Mon Apr 19 09:12:06 2021

Number of Points = 3634
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.626712	0.024649	0.000000	0.000025	0.308664

2.355973	0.078524	0.005005	0.000075	0.308686
2.344595	0.078936	0.010010	0.000077	0.308678
2.562756	0.037347	0.015014	0.000037	0.308669
2.771611	-0.000603	0.020019	-0.000002	0.308669
2.403563	0.066873	0.025024	0.000066	0.308671
2.382049	0.073801	0.030029	0.000070	0.308685
2.461226	0.057197	0.035034	0.000056	0.308675
2.553371	0.038921	0.040038	0.000039	0.308667
2.370142	0.073799	0.045043	0.000073	0.308675
2.495573	0.049533	0.050048	0.000049	0.308667
2.669342	0.018919	0.055053	0.000017	0.308672
2.380863	0.072088	0.060058	0.000071	0.308675
2.481619	0.054132	0.065062	0.000052	0.308677
2.721661	0.009042	0.070067	0.000008	0.308669
2.517988	0.046660	0.075072	0.000046	0.308672
2.579536	0.036749	0.080077	0.000034	0.308678
2.687007	-0.030332	0.085082	0.000014	0.308455
2.020343	0.071236	0.090086	0.000138	0.308363
2.152175	0.048137	0.095091	0.000114	0.308366
2.530563	-0.024662	0.100096	0.000043	0.308347
2.420181	-0.001561	0.105101	0.000064	0.308361
2.272954	0.022454	0.110106	0.000091	0.308348
2.366526	0.004235	0.115110	0.000074	0.308342
2.359745	-0.027079	0.120115	0.000075	0.308189
1.979562	0.017770	0.125120	0.000146	0.308075
2.002874	0.015085	0.130125	0.000142	0.308083
2.419846	-0.065063	0.135130	0.000064	0.308062
2.875668	-0.152406	0.140134	-0.000020	0.308040
2.623825	-0.134000	0.145139	0.000027	0.307912
2.303377	-0.116381	0.150144	0.000086	0.307721
2.437251	-0.138995	0.155149	0.000061	0.307728
2.286557	-0.112513	0.160154	0.000089	0.307724
2.348476	-0.133074	0.165158	0.000078	0.307680
2.654921	-0.246051	0.170163	0.000021	0.307410
2.129556	-0.149921	0.175168	0.000119	0.307413
2.473597	-0.211108	0.180173	0.000055	0.307419
2.547949	-0.256304	0.185178	0.000041	0.307270
2.171375	-0.224653	0.190182	0.000111	0.307096
2.032650	-0.199127	0.195187	0.000137	0.307098
2.218154	-0.236596	0.200192	0.000103	0.307080
2.206162	-0.283648	0.205197	0.000105	0.306848
1.963464	-0.247208	0.210202	0.000150	0.306811
2.231091	-0.297129	0.215206	0.000100	0.306805
2.171388	-0.327890	0.220211	0.000112	0.306608
2.149098	-0.353594	0.225216	0.000116	0.306468
2.300276	-0.380124	0.230221	0.000088	0.306472
2.628610	-0.487691	0.235226	0.000027	0.306246
2.525086	-0.489154	0.240230	0.000046	0.306150
2.352242	-0.457440	0.245235	0.000078	0.306151
2.229570	-0.500894	0.250240	0.000101	0.305840
2.195383	-0.492131	0.255245	0.000108	0.305852
2.108742	-0.500635	0.260250	0.000124	0.305737
2.280810	-0.563532	0.265254	0.000092	0.305587
2.379295	-0.579991	0.270259	0.000073	0.305593
2.080167	-0.598103	0.275264	0.000129	0.305250
2.120796	-0.606221	0.280269	0.000122	0.305246
2.296487	-0.677045	0.285274	0.000089	0.305062
2.252184	-0.697024	0.290278	0.000097	0.304928
2.361881	-0.741505	0.295283	0.000077	0.304812
2.229650	-0.765371	0.300288	0.000102	0.304584
2.540020	-0.834188	0.305293	0.000044	0.304525
2.551967	-0.885012	0.310298	0.000042	0.304293
2.300725	-0.851268	0.315302	0.000089	0.304237
2.438124	-0.934378	0.320307	0.000063	0.303960
2.020406	-0.869123	0.325312	0.000141	0.303909
2.038645	-0.923174	0.330317	0.000138	0.303667
1.983276	-0.923520	0.335322	0.000148	0.303617
1.875899	-0.961913	0.340326	0.000168	0.303341
1.844554	-0.962281	0.345331	0.000174	0.303312
2.129261	-1.069972	0.350336	0.000121	0.303044
2.213712	-1.105645	0.355341	0.000105	0.302947
2.271054	-1.165650	0.360346	0.000095	0.302710
2.189138	-1.184252	0.365350	0.000110	0.302550
2.353976	-1.245570	0.370355	0.000079	0.302400
2.127517	-1.258614	0.375360	0.000122	0.302140
1.919807	-1.235284	0.380365	0.000160	0.302071
1.792079	-1.269405	0.385370	0.000184	0.301796
1.791017	-1.290004	0.390374	0.000185	0.301696
1.780561	-1.335816	0.395379	0.000187	0.301467
1.679030	-1.354742	0.400384	0.000205	0.301287
1.998067	-1.440872	0.405389	0.000146	0.301152
2.077093	-1.517415	0.410394	0.000132	0.300852
1.811142	-1.487957	0.415398	0.000181	0.300762
2.111700	-1.576948	0.420403	0.000125	0.300596
1.644076	-1.544409	0.425408	0.000212	0.300343
1.639228	-1.570293	0.430413	0.000213	0.300214
1.477294	-1.595926	0.435418	0.000244	0.299948
1.609540	-1.660555	0.440422	0.000219	0.299752
1.377166	-1.645109	0.445427	0.000262	0.299623
1.440789	-1.718338	0.450432	0.000251	0.299325
1.495502	-1.760668	0.455437	0.000240	0.299168
1.178300	-1.736663	0.460442	0.000299	0.299005
1.030742	-1.771417	0.465446	0.000327	0.298706
1.269904	-1.845708	0.470451	0.000283	0.298557
1.294362	-1.887551	0.475456	0.000278	0.298375
1.191102	-1.927005	0.480461	0.000297	0.298093
1.288529	-1.983795	0.485466	0.000279	0.297903
1.300924	-2.025832	0.490470	0.000277	0.297709
1.323051	-2.086553	0.495475	0.000273	0.297433
1.005894	-2.079037	0.500480	0.000332	0.297189
1.191858	-2.150534	0.505485	0.000298	0.297005
1.157412	-2.183938	0.510490	0.000304	0.296812
1.134391	-2.245935	0.515494	0.000308	0.296489
1.297654	-2.315459	0.520499	0.000278	0.296294
1.007108	-2.306297	0.525504	0.000332	0.296081
0.784275	-2.309307	0.530509	0.000374	0.295868
1.051096	-2.405971	0.535514	0.000324	0.295632
1.252941	-2.493675	0.540518	0.000287	0.295382
0.801241	-2.457920	0.545523	0.000371	0.295155
0.345516	-2.420971	0.550528	0.000456	0.294929
-0.277117	-2.371438	0.555533	0.000572	0.294617
-0.604488	-2.349741	0.560538	0.000633	0.294431
-0.822169	-2.346497	0.565542	0.000673	0.294252
-1.002731	-2.368149	0.570547	0.000707	0.293984
-1.173744	-2.385874	0.575552	0.000739	0.293743
-1.858266	-2.290720	0.580557	0.000866	0.293599
-2.252735	-2.264471	0.585562	0.000940	0.293374
-2.434097	-2.272700	0.590566	0.000974	0.293171
-2.748458	-2.236986	0.595571	0.001032	0.293065
-2.979983	-2.262214	0.600576	0.001075	0.292732
-3.097884	-2.267161	0.605581	0.001097	0.292602
-3.704707	-2.191102	0.610586	0.001210	0.292432
-3.464638	-2.286735	0.615590	0.001166	0.292174
-3.596116	-2.284426	0.620595	0.001190	0.292067
-4.250986	-2.219878	0.625600	0.001312	0.291797
-4.421400	-2.206840	0.630605	0.001344	0.291708
-4.597200	-2.220917	0.635610	0.001377	0.291479
-4.813200	-2.217061	0.640614	0.001417	0.291303
-5.024266	-2.204188	0.645619	0.001456	0.291176
-5.207835	-2.217960	0.650624	0.001491	0.290941
-5.619780	-2.159319	0.655629	0.001567	0.290860
-5.890529	-2.154981	0.660634	0.001618	0.290637
-5.834038	-2.173981	0.665638	0.001607	0.290593
-5.815081	-2.240271	0.670643	0.001604	0.290280
-6.379923	-2.146934	0.675648	0.001709	0.290233
-6.315024	-2.219778	0.680653	0.001697	0.289928
-6.610695	-2.171998	0.685658	0.001752	0.289898
-6.905552	-2.179087	0.690662	0.001807	0.289595
-6.758764	-2.212475	0.695667	0.001780	0.289561
-6.767710	-2.265090	0.700672	0.001781	0.289290
-7.289624	-2.179842	0.705677	0.001879	0.289241
-7.588770	-2.179786	0.710682	0.001934	0.288969
-7.846493	-2.141447	0.715686	0.001982	0.288926
-7.948540	-2.174020	0.720691	0.002001	0.288670
-8.373146	-2.103715	0.725696	0.002081	0.288635
-8.417414	-2.154624	0.730701	0.002089	0.288339
-8.382010	-2.163199	0.735706	0.002082	0.288328
-9.154863	-2.074400	0.740710	0.002226	0.288068
-9.419900	-2.025608	0.745715	0.002276	0.288071
-9.319878	-2.090072	0.750720	0.002257	0.287838
-9.575251	-2.066397	0.755725	0.002305	0.287724
-9.784918	-2.046998	0.760730	0.002344	0.287629
-9.933137	-2.065222	0.765734	0.002371	0.287402
-9.767037	-2.096015	0.770739	0.002340	0.287399
-10.215305	-2.078811	0.775744	0.002424	0.287074
-10.404623	-2.040848	0.780749	0.002459	0.287092
-10.507437	-2.059827	0.785754	0.002478	0.286902
-11.060187	-1.980162	0.790758	0.002581	0.286797
-10.752604	-2.048042	0.795763	0.002524	0.286736
-10.797821	-2.095192	0.800768	0.002533	0.286456
-10.866684	-2.079996	0.805773	0.002546	0.286469
-11.453712	-2.025170	0.810778	0.002655	0.286207
-11.668919	-1.994918	0.815782	0.002695	0.286162
-11.171778	-2.109711	0.820787	0.002602	0.286038
-11.647238	-2.064932	0.825792	0.002691	0.285827
-11.854778	-2.022757	0.830797	0.002730	0.285849
-11.881208	-2.068869	0.835802	0.002735	0.285591
-11.885420	-2.070644	0.840806	0.002736	0.285578
-12.178541	-2.053672	0.845811	0.002790	0.285394
-12.617339	-2.002501	0.850816	0.002872	0.285248
-12.464468	-2.035423	0.855821	0.002843	0.285222
-13.018964	-1.990156	0.860826	0.002947	0.284940
-12.835517	-2.025682	0.865830	0.002913	0.284929
-12.875239	-2.052178	0.870835	0.002920	0.284757
-13.597126	-1.951560	0.875840	0.003054	0.284601
-12.966148	-2.070620	0.880845	0.002937	0.284579
-13.297793	-2.063025	0.885850	0.002999	0.284310
-13.453130	-2.036829	0.890854	0.003028	0.284300
-13.174631	-2.124232	0.895859	0.002976	0.284112
-13.815308	-2.037039	0.900864	0.003095	0.283963
-13.834385	-2.037666	0.905869	0.003099	0.283942
-14.158162	-2.034467	0.910874	0.003159	0.283658
-14.239082	-2.021490	0.915878	0.003174	0.283649
-13.700116	-2.154641	0.920883	0.003074	0.283469
-14.214296	-2.091399	0.925888	0.003170	0.283314
-14.257975	-2.091472	0.930893	0.003178	0.283273
-14.441180	-2.104684	0.935898	0.003212	0.283035
-14.844235	-2.031560	0.940902	0.003287	0.283034
-14.982559	-2.049491	0.945907	0.003313	0.282813
-15.657641	-1.947612	0.950912	0.003439	0.282706
-14.948987	-2.081001	0.955917	0.003307	0.282683
-15.365935	-2.062008	0.960922	0.003385	0.282391
-15.504589	-2.037767	0.965926	0.003410	0.282386
-15.584821	-2.051077	0.970931	0.003425	0.282243
-16.304828	-1.952501	0.975936	0.003560	0.282077
-16.387183	-1.935594	0.980941	0.003575	0.282087
-16.325253	-1.989090	0.985946	0.003563	0.281870
-16.295447	-2.012971	0.990950	0.003558	0.281775
-16.278854	-2.023154	0.995955	0.003555	0.281738
-16.757195	-1.991863	1.000960	0.003644	0.281451
-16.633657	-2.014347	1.005965	0.003621	0.281451
-16.922783	-1.987719	1.010970	0.003675	0.281317
-17.429952	-1.929168	1.015974	0.003769	0.281144
-16.853022	-2.033079	1.020979	0.003662	0.281148
-17.439920	-1.972272	1.025984	0.003771	0.280912
-17.947670	-1.893858	1.030989	0.003866	0.280840
-17.691438	-1.940413	1.035994	0.003818	0.280840
-17.711948	-1.978818	1.040998	0.003822	0.280622
-18.056509	-1.918722	1.046003	0.003886	0.280609
-18.099454	-1.920855	1.051008	0.003894	0.280557
-18.062764	-1.984213	1.056013	0.003888	0.280265
-18.351411	-1.930118	1.061018	0.003941	0.280273
-18.859416	-1.858995	1.066022	0.004036	0.280163
-18.587377	-1.947639	1.071027	0.003985	0.279960
-18.646907	-1.939878	1.076032	0.003996	0.279944
-18.838860	-1.938666	1.081037	0.004032	0.279769
-19.196665	-1.900921	1.086042	0.004099	0.279628
-18.884938	-1.960833	1.091046	0.004041	0.279611
-19.075153	-1.967659	1.096051	0.004076	0.279396
-19.901630	-1.829763	1.101056	0.004230	0.279332
-19.430343	-1.915575	1.106061	0.004143	0.279331
-19.457910	-1.969906	1.111066	0.004148	0.279023
-19.985684	-1.881314	1.116070	0.004246	0.278984
-19.471830	-1.984218	1.121075	0.004151	0.278935
-19.304865	-2.069358	1.126080	0.004120	0.278650
-19.560849	-2.020781	1.131085	0.004167	0.278661
-20.015946	-1.974273	1.136090	0.004252	0.278472
-19.891492	-2.024441	1.141094	0.004229	0.278329
-19.922233	-2.017976	1.146099	0.004235	0.278333
-20.482241	-1.969364	1.151104	0.004339	0.278056
-20.408883	-1.981458	1.156109	0.004325	0.278062
-20.454051	-1.999674	1.161114	0.004334	0.277924
-21.093512	-1.923300	1.166118	0.004453	0.277716
-20.497397	-2.031421	1.171123	0.004342	0.277717
-20.495269	-2.079885	1.176128	0.004342	0.277466
-21.024838	-1.996903	1.181133	0.004440	0.277397
-21.484265	-1.920150	1.186138	0.004526	0.277361
-21.048609	-2.056039	1.191142	0.004445	0.277065
-20.995164	-2.063770	1.196147	0.004435	0.277075
-21.617562	-1.985691	1.201152	0.004551	0.276891
-22.079212	-1.919608	1.206157	0.004637	0.276798
-21.910655	-1.948744	1.211162	0.004605	0.276805
-22.133409	-1.966816	1.216166	0.004647	0.276499
-22.181790	-1.963334	1.221171	0.004656	0.276471
-21.832406	-2.044608	1.226176	0.004591	0.276377
-21.999606	-2.058912	1.231181	0.004622	0.276143
-22.396762	-1.985463	1.236186	0.004696	0.276149
-22.366314	-2.035589	1.241190	0.004691	0.275915
-22.580699	-2.010013	1.246195	0.004730	0.275844
-22.839069	-1.970190	1.251200	0.004779	0.275807
-23.015939	-1.978147	1.256205	0.004812	0.275596
-22.720692	-2.032104	1.261210	0.004757	0.275594
-22.985276	-2.018960	1.266214	0.004806	0.275410
-23.303891	-1.991490	1.271219	0.004865	0.275250
-23.024603	-2.044184	1.276224	0.004813	0.275239
-23.132331	-2.081494	1.281229	0.004834	0.274940
-23.889010	-1.945339	1.286234	0.004974	0.274932
-23.758178	-1.993145	1.291238	0.004950	0.274805
-23.922549	-2.000089	1.296243	0.004981	0.274611
-23.730491	-2.038823	1.301248	0.004945	0.274590
-23.848888	-2.061050	1.306253	0.004967	0.274359
-23.844113	-2.072472	1.311258	0.004966	0.274303
-23.937600	-2.080502	1.316262	0.004984	0.274171
-24.581608	-2.000041	1.321267	0.005104	0.273977
-24.246171	-2.065524	1.326272	0.005041	0.273953
-24.574393	-2.049940	1.331277	0.005102	0.273720
-25.042108	-1.974358	1.336282	0.005190	0.273669
-25.108758	-1.973807	1.341286	0.005202	0.273608
-25.250947	-1.995281	1.346291	0.005229	0.273357
-25.852940	-1.884546	1.351296	0.005341	0.273364
-25.705603	-1.938078	1.356301	0.005313	0.273222
-25.461788	-2.013102	1.361306	0.005268	0.273059
-25.354665	-2.034919	1.366310	0.005248	0.273046
-25.505398	-2.060958	1.371315	0.005276	0.272762
-25.235936	-2.122572	1.376320	0.005226	0.272695
-25.489244	-2.100990	1.381325	0.005273	0.272565
-26.445284	-1.955828	1.386330	0.005451	0.272412
-26.297974	-1.985051	1.391334	0.005424	0.272399
-26.293826	-2.032385	1.396339	0.005423	0.272151
-26.659594	-1.980159	1.401344	0.005491	0.272075
-26.451264	-2.030755	1.406349	0.005453	0.272007
-26.597842	-2.044471	1.411354	0.005480	0.271792
-26.830298	-2.003880	1.416358	0.005523	0.271783
-27.218746	-1.968617	1.421363	0.005596	0.271594
-27.479752	-1.944872	1.426368	0.005644	0.271467
-27.501023	-1.939874	1.431373	0.005648	0.271473
-27.269924	-2.036174	1.436378	0.005605	0.271183
-27.634123	-1.975653	1.441382	0.005673	0.271152
-27.246732	-2.064384	1.446387	0.005601	0.271054
-27.484921	-2.066266	1.451392	0.005645	0.270813
-27.021010	-2.151732	1.456397	0.005559	0.270807
-27.293227	-2.145254	1.461402	0.005610	0.270576
-27.716834	-2.070501	1.466406	0.005689	0.270564
-27.497010	-2.147281	1.471411	0.005648	0.270366
-27.794720	-2.123356	1.476416	0.005703	0.270204
-28.356370	-2.025091	1.481421	0.005808	0.270183
-28.649824	-2.021367	1.486426	0.005863	0.269917
-28.730441	-2.008888	1.491430	0.005878	0.269905
-28.783276	-2.029550	1.496435	0.005888	0.269742
-29.261050	-1.971110	1.501440	0.005977	0.269589
-29.017938	-2.017530	1.506445	0.005931	0.269577
-29.261072	-2.019329	1.511450	0.005977	0.269330
-29.953213	-1.893736	1.516454	0.006106	0.269328
-29.900498	-1.913609	1.521459	0.006096	0.269272
-30.055043	-1.939414	1.526464	0.006125	0.268982
-29.863134	-1.973290	1.531469	0.006089	0.268987
-30.011662	-1.972193	1.536474	0.006117	0.268847
-30.822940	-1.856133	1.541478	0.006268	0.268677
-30.527697	-1.904916	1.546483	0.006213	0.268704
-30.735743	-1.907516	1.551488	0.006252	0.268486
-31.110831	-1.862399	1.556493	0.006321	0.268361
-30.852836	-1.909364	1.561498	0.006273	0.268360
-30.781092	-1.965569	1.566502	0.006260	0.268127
-31.357379	-1.871328	1.571507	0.006367	0.268070
-31.210360	-1.899735	1.576512	0.006340	0.268060
-31.228667	-1.957405	1.581517	0.006344	0.267730
-31.396389	-1.927350	1.586522	0.006375	0.267728
-31.761399	-1.876466	1.591526	0.006443	0.267644
-31.495910	-1.966796	1.596531	0.006394	0.267416
-31.492793	-1.970459	1.601536	0.006393	0.267399
-32.117860	-1.887916	1.606541	0.006509	0.267230
-32.203215	-1.898824	1.611546	0.006525	0.267086
-32.026287	-1.931992	1.616550	0.006492	0.267081
-32.196839	-1.941150	1.621555	0.006524	0.266863
-32.511265	-1.896086	1.626560	0.006583	0.266797
-31.706542	-2.057530	1.631565	0.006433	0.266715
-32.062325	-2.041690	1.636570	0.006499	0.266449
-32.588243	-1.946571	1.641574	0.006597	0.266446
-32.551705	-1.987191	1.646579	0.006591	0.266261
-32.860487	-1.953006	1.651584	0.006648	0.266141
-32.700369	-1.986835	1.656589	0.006618	0.266115
-32.934499	-1.995512	1.661594	0.006662	0.265836
-33.070968	-1.974450	1.666598	0.006687	0.265815
-32.962614	-2.018712	1.671603	0.006667	0.265681
-33.339659	-1.972355	1.676608	0.006738	0.265560
-33.035345	-2.028682	1.681613	0.006681	0.265554
-33.372345	-2.027669	1.686618	0.006744	0.265225
-34.086747	-1.898549	1.691622	0.006877	0.265220
-33.896348	-1.953826	1.696627	0.006841	0.265107
-34.066075	-1.959099	1.701632	0.006873	0.264909
-34.099775	-1.952684	1.706637	0.006879	0.264911
-34.171436	-1.986039	1.711642	0.006893	0.264657
-34.545775	-1.930632	1.716646	0.006962	0.264587
-34.722908	-1.904603	1.721651	0.006995	0.264553
-34.899013	-1.919437	1.726656	0.007028	0.264296
-34.787686	-1.937509	1.731661	0.007008	0.264308
-34.972532	-1.932658	1.736666	0.007042	0.264150
-35.545448	-1.862276	1.741670	0.007149	0.263964
-34.886132	-1.980882	1.746675	0.007026	0.263971
-35.078186	-1.993841	1.751680	0.007062	0.263708
-35.560276	-1.916765	1.756685	0.007152	0.263649
-35.547813	-1.931477	1.761690	0.007149	0.263581
-35.910273	-1.911092	1.766694	0.007217	0.263330
-35.579186	-1.970642	1.771699	0.007155	0.263334
-36.217194	-1.884720	1.776704	0.007274	0.263168
-35.660411	-2.010885	1.781709	0.007171	0.263030
-35.723719	-2.001707	1.786714	0.007182	0.263017
-36.316463	-1.952979	1.791718	0.007293	0.262691
-36.670445	-1.884922	1.796723	0.007359	0.262711
-36.313006	-1.975209	1.801728	0.007292	0.262572
-36.857289	-1.907955	1.806733	0.007394	0.262396
-36.753850	-1.927281	1.811738	0.007374	0.262393
-37.089575	-1.914090	1.816742	0.007437	0.262129
-37.009220	-1.937962	1.821747	0.007422	0.262077
-37.280053	-1.898534	1.826752	0.007473	0.262023
-37.282293	-1.941365	1.831757	0.007473	0.261783
-36.960924	-2.001607	1.836762	0.007413	0.261773
-37.590506	-1.925814	1.841766	0.007530	0.261559
-37.386953	-1.985197	1.846771	0.007493	0.261435
-37.298701	-2.006787	1.851776	0.007476	0.261404
-37.675473	-1.987814	1.856781	0.007546	0.261129
-37.610600	-2.000871	1.861786	0.007534	0.261121
-37.856463	-1.993902	1.866790	0.007580	0.260912
-37.549136	-2.067066	1.871795	0.007523	0.260816
-38.331018	-1.932567	1.876800	0.007669	0.260772
-38.366524	-1.960658	1.881805	0.007675	0.260580
-38.291228	-1.972494	1.886810	0.007661	0.260590
-39.046667	-1.877950	1.891814	0.007802	0.260352
-38.774208	-1.946095	1.896819	0.007751	0.260248
-38.754421	-1.957480	1.901824	0.007748	0.260204
-38.910725	-1.980530	1.906829	0.007777	0.259917
-39.371073	-1.895129	1.911834	0.007863	0.259926
-39.396101	-1.924527	1.916838	0.007867	0.259737
-39.592560	-1.912238	1.921843	0.007904	0.259606
-39.922818	-1.853722	1.926848	0.007965	0.259597
-39.999444	-1.882991	1.931853	0.007980	0.259356
-39.817121	-1.923081	1.936858	0.007946	0.259317
-40.321171	-1.844217	1.941862	0.008040	0.259245
-40.563840	-1.846028	1.946867	0.008085	0.258988
-40.591069	-1.841573	1.951872	0.008090	0.258985
-40.214106	-1.939586	1.956877	0.008020	0.258820
-40.773956	-1.863409	1.961882	0.008124	0.258676
-40.891779	-1.842001	1.966886	0.008146	0.258675
-40.424671	-1.974517	1.971891	0.008059	0.258409
-40.948987	-1.891581	1.976896	0.008157	0.258339
-41.058355	-1.885090	1.981901	0.008177	0.258263
-40.916097	-1.949046	1.986906	0.008151	0.258049
-40.583994	-2.014644	1.991910	0.008089	0.258020
-40.898966	-2.004481	1.996915	0.008148	0.257755
-41.423347	-1.924836	2.001920	0.008246	0.257666

-41.934700	-1.879705	2.011917	0.008341	0.257396
-41.659779	-1.965745	2.021914	0.008290	0.257193
-41.798471	-1.964992	2.031910	0.008316	0.257055
-42.172764	-1.943909	2.041907	0.008385	0.256789
-41.944864	-1.990288	2.051904	0.008343	0.256761
-42.445847	-1.955117	2.061901	0.008436	0.256445
-42.429623	-1.959169	2.071898	0.008434	0.256438
-42.510751	-1.965404	2.081894	0.008449	0.256319
-42.464338	-2.009747	2.091891	0.008440	0.256115
-42.817734	-1.942418	2.101888	0.008506	0.256132
-43.192611	-1.872483	2.111885	0.008576	0.256141
-42.866403	-1.933499	2.121882	0.008515	0.256131
-43.192682	-1.928047	2.131878	0.008576	0.255826
-43.112364	-1.945967	2.141875	0.008561	0.255807
-42.966652	-1.972920	2.151872	0.008534	0.255804
-42.947456	-1.977324	2.161869	0.008531	0.255798
-42.853032	-1.993407	2.171866	0.008513	0.255804
-42.729867	-2.014267	2.181862	0.008490	0.255812
-43.212740	-1.925630	2.191859	0.008580	0.255816
-42.830332	-1.997415	2.201856	0.008509	0.255803
-42.972369	-1.913863	2.211853	0.008536	0.256129
-42.699657	-1.962856	2.221850	0.008485	0.256132
-42.581269	-1.986579	2.231846	0.008463	0.256119
-42.554806	-1.991367	2.241843	0.008458	0.256119
-42.609876	-1.981718	2.251840	0.008469	0.256116
-42.507565	-1.976345	2.261837	0.008450	0.256252
-42.307629	-1.979641	2.271834	0.008413	0.256438
-42.771833	-1.892637	2.281830	0.008499	0.256452
-42.457601	-1.941807	2.291827	0.008441	0.256497
-42.492569	-1.885636	2.301824	0.008447	0.256777
-42.460445	-1.890809	2.311821	0.008441	0.256780
-42.145693	-1.916185	2.321818	0.008383	0.256960
-41.962187	-1.931732	2.331814	0.008349	0.257060
-41.670541	-1.979242	2.341811	0.008295	0.257091
-41.522629	-1.956071	2.351808	0.008267	0.257372
-41.531112	-1.953585	2.361805	0.008269	0.257377
-40.920173	-2.021263	2.371802	0.008155	0.257621
-41.014146	-1.992406	2.381798	0.008173	0.257687
-40.647169	-2.032056	2.391795	0.008105	0.257839
-40.930255	-1.945073	2.401792	0.008157	0.258037
-41.059113	-1.898304	2.411789	0.008181	0.258168
-40.935853	-1.890406	2.421786	0.008158	0.258337
-40.273238	-1.978090	2.431782	0.008035	0.258521
-39.863107	-2.031604	2.441779	0.007959	0.258639
-40.112567	-1.949162	2.451776	0.008005	0.258846
-39.335412	-2.073992	2.461773	0.007861	0.258938
-39.338091	-2.028712	2.471770	0.007861	0.259188
-39.380866	-2.003671	2.481766	0.007870	0.259284
-39.236314	-1.983674	2.491763	0.007843	0.259542
-39.066368	-2.003584	2.501760	0.007811	0.259603
-38.341679	-2.084811	2.511757	0.007676	0.259884
-38.868147	-1.964163	2.521754	0.007774	0.260022
-38.192197	-2.052695	2.531750	0.007649	0.260214
-38.066517	-2.033581	2.541747	0.007625	0.260447
-38.169331	-1.994005	2.551744	0.007645	0.260562
-38.201540	-1.944116	2.561741	0.007651	0.260807
-38.231357	-1.906787	2.571738	0.007656	0.260983
-37.723993	-1.968046	2.581734	0.007562	0.261155
-37.503128	-1.957882	2.591731	0.007521	0.261433
-37.303321	-1.958832	2.601728	0.007484	0.261629
-37.093490	-1.964658	2.611725	0.007445	0.261808
-37.157425	-1.908387	2.621722	0.007457	0.262054
-36.791314	-1.929230	2.631718	0.007389	0.262306
-36.915845	-1.867288	2.641715	0.007412	0.262522
-36.779789	-1.852151	2.651712	0.007387	0.262742
-36.456592	-1.855503	2.661709	0.007326	0.263047
-36.225161	-1.857084	2.671706	0.007283	0.263269
-36.137484	-1.828339	2.681702	0.007267	0.263515
-35.801979	-1.848289	2.691699	0.007205	0.263740
-35.697472	-1.825150	2.701696	0.007185	0.263971
-34.835460	-1.924908	2.711693	0.007025	0.264283
-34.905102	-1.876505	2.721690	0.007038	0.264478
-34.718678	-1.870640	2.731686	0.007004	0.264696
-34.456600	-1.877261	2.741683	0.006955	0.264920
-33.907888	-1.920672	2.751680	0.006853	0.265227
-34.044704	-1.852742	2.761677	0.006878	0.265462
-33.467809	-1.921686	2.771674	0.006771	0.265658
-33.171935	-1.944908	2.781670	0.006716	0.265824
-33.066834	-1.905770	2.791667	0.006696	0.266141
-32.716710	-1.933648	2.801664	0.006631	0.266335
-32.675424	-1.900325	2.811661	0.006624	0.266556
-32.250705	-1.934296	2.821658	0.006545	0.266791
-31.938498	-1.940601	2.831654	0.006487	0.267064
-31.985075	-1.890770	2.841651	0.006495	0.267288
-31.745526	-1.893921	2.851648	0.006451	0.267506
-31.108599	-1.972341	2.861645	0.006333	0.267708
-30.700770	-1.987416	2.871642	0.006257	0.268028
-30.530470	-1.988440	2.881638	0.006225	0.268189
-30.254100	-2.006030	2.891635	0.006174	0.268365
-29.792994	-2.039888	2.901632	0.006088	0.268634
-30.051565	-1.949360	2.911629	0.006136	0.268868
-29.620590	-1.991422	2.921626	0.006056	0.269063
-29.593647	-1.950538	2.931622	0.006051	0.269309
-29.023320	-2.006065	2.941619	0.005945	0.269567
-28.902516	-1.990480	2.951616	0.005923	0.269769
-28.780626	-1.972381	2.961613	0.005900	0.269984
-28.327078	-2.010800	2.971610	0.005816	0.270220
-28.453550	-1.928370	2.981606	0.005839	0.270538
-28.571495	-1.868055	2.991603	0.005861	0.270745
-28.008537	-1.933512	3.001600	0.005756	0.270942
-27.946936	-1.899134	3.011597	0.005745	0.271185
-27.615054	-1.909729	3.021594	0.005683	0.271450
-27.209076	-1.932562	3.031590	0.005608	0.271722
-26.585730	-2.011247	3.041587	0.005492	0.271906
-25.915520	-2.106665	3.051584	0.005367	0.272047
-25.956072	-2.038586	3.061581	0.005375	0.272369
-25.548220	-2.077086	3.071578	0.005299	0.272558
-25.521419	-2.046186	3.081574	0.005294	0.272748
-24.873148	-2.113798	3.091571	0.005174	0.273014
-24.987489	-2.051635	3.101568	0.005195	0.273233
-24.784141	-2.056174	3.111565	0.005157	0.273404
-24.992713	-1.971643	3.121562	0.005196	0.273650
-25.004391	-1.909881	3.131558	0.005198	0.273965
-24.739514	-1.910464	3.141555	0.005149	0.274216
-24.510281	-1.907039	3.151552	0.005106	0.274454
-23.975121	-1.965437	3.161549	0.005007	0.274659
-23.806653	-1.946414	3.171546	0.004976	0.274920
-23.608657	-1.925356	3.181542	0.004939	0.275220
-23.247237	-1.944640	3.191539	0.004872	0.275464
-23.139302	-1.926568	3.201536	0.004852	0.275661
-22.989526	-1.918096	3.211533	0.004824	0.275848
-22.640252	-1.931669	3.221530	0.004759	0.276110
-22.655819	-1.871544	3.231526	0.004762	0.276410
-22.180271	-1.910464	3.241523	0.004673	0.276658
-22.313355	-1.838045	3.251520	0.004698	0.276910
-22.192323	-1.811486	3.261517	0.004676	0.277163
-21.843614	-1.825801	3.271514	0.004611	0.277419
-21.880753	-1.764773	3.281510	0.004618	0.277702
-21.416472	-1.787653	3.291507	0.004531	0.278022
-21.588195	-1.705793	3.301504	0.004564	0.278285
-21.020030	-1.755761	3.311501	0.004458	0.278562
-21.387910	-1.630427	3.321498	0.004526	0.278865
-20.978141	-1.646974	3.331494	0.004450	0.279165
-21.025995	-1.579691	3.341491	0.004459	0.279469
-20.349070	-1.649907	3.351488	0.004333	0.279742
-20.309704	-1.600180	3.361485	0.004326	0.280036
-20.391306	-1.520793	3.371482	0.004341	0.280369
-20.131439	-1.510980	3.381478	0.004293	0.280663
-19.903029	-1.499166	3.391475	0.004250	0.280937
-19.834013	-1.448108	3.401472	0.004238	0.281265
-19.565211	-1.436437	3.411469	0.004188	0.281576
-19.613249	-1.359891	3.421466	0.004197	0.281924
-19.470860	-1.322574	3.431462	0.004170	0.282248
-18.982479	-1.348810	3.441459	0.004079	0.282568
-18.912806	-1.292442	3.451456	0.004066	0.282921
-18.318977	-1.337347	3.461453	0.003956	0.283243
-17.545954	-1.419826	3.471450	0.003812	0.283539
-16.829174	-1.495591	3.481446	0.003679	0.283817
-17.033493	-1.398897	3.491443	0.003717	0.284120
-17.036004	-1.338375	3.501440	0.003717	0.284426
-17.234734	-1.240392	3.511437	0.003754	0.284740
-16.914790	-1.234271	3.521434	0.003695	0.285066
-16.719404	-1.201338	3.531430	0.003659	0.285413
-16.258742	-1.226316	3.541427	0.003573	0.285710
-15.257956	-1.355179	3.551424	0.003387	0.285979
-14.616513	-1.421778	3.561421	0.003267	0.286231
-14.093376	-1.469384	3.571418	0.003170	0.286471
-13.921312	-1.446075	3.581414	0.003138	0.286746
-13.801639	-1.411000	3.591411	0.003116	0.287033
-13.969680	-1.325378	3.601408	0.003147	0.287310
-13.638928	-1.326961	3.611405	0.003086	0.287604
-12.976861	-1.392205	3.621402	0.002963	0.287881
-12.292750	-1.465462	3.631398	0.002835	0.288137
-11.527184	-1.569532	3.641395	0.002693	0.288313
-11.110565	-1.581568	3.651392	0.002616	0.288632
-10.629964	-1.633416	3.661389	0.002526	0.288810
-10.393475	-1.644727	3.671386	0.002482	0.288968
-9.928223	-1.666062	3.681382	0.002396	0.289285
-9.303831	-1.756727	3.691379	0.002280	0.289398
-9.012141	-1.775348	3.701376	0.002225	0.289570
-8.871654	-1.751793	3.711373	0.002199	0.289815
-8.313790	-1.833992	3.721370	0.002096	0.289910
-8.156920	-1.800852	3.731366	0.002066	0.290218
-7.825684	-1.843229	3.741363	0.002005	0.290306
-7.375509	-1.877258	3.751360	0.001921	0.290544
-7.327383	-1.861880	3.761357	0.001912	0.290664
-7.084894	-1.875809	3.771354	0.001867	0.290813
-7.052760	-1.836014	3.781350	0.001861	0.291040
-6.631604	-1.894334	3.791347	0.001783	0.291130
-6.217503	-1.912239	3.801344	0.001706	0.291415
-6.334896	-1.874508	3.811341	0.001728	0.291496
-6.265600	-1.831269	3.821338	0.001715	0.291772
-6.182433	-1.809685	3.831334	0.001700	0.291954
-5.687037	-1.876777	3.841331	0.001608	0.292067
-5.188708	-1.905786	3.851328	0.001515	0.292372
-5.002497	-1.921637	3.861325	0.001480	0.292460
-5.534052	-1.774246	3.871322	0.001579	0.292711
-5.192329	-1.784117	3.881318	0.001516	0.292969
-4.996780	-1.785453	3.891315	0.001479	0.293137
-5.307229	-1.685297	3.901312	0.001537	0.293353
-4.957709	-1.686801	3.911309	0.001472	0.293658
-4.400525	-1.747834	3.921306	0.001369	0.293856
-3.897088	-1.807731	3.931302	0.001275	0.294011
-4.176729	-1.695743	3.941299	0.001327	0.294312
-4.261161	-1.633871	3.951296	0.001343	0.294540
-4.017646	-1.631917	3.961293	0.001298	0.294766
-3.484615	-1.689224	3.971290	0.001198	0.294960
-3.338281	-1.660656	3.981286	0.001171	0.295230
-3.455910	-1.573222	3.991283	0.001193	0.295553
-3.225026	-1.573831	4.001280	0.001150	0.295755
-3.092364	-1.554841	4.011277	0.001126	0.295966
-3.156175	-1.489152	4.021274	0.001138	0.296230
-3.121781	-1.439087	4.031270	0.001131	0.296504
-3.035414	-1.391388	4.041267	0.001115	0.296813
-2.471433	-1.440159	4.051264	0.001010	0.297075
-2.117388	-1.445500	4.061261	0.000945	0.297361
-1.925961	-1.424092	4.071258	0.000909	0.297634
-1.647590	-1.417574	4.081254	0.000857	0.297912
-1.677641	-1.354605	4.091251	0.000863	0.298190
-1.406819	-1.351467	4.101248	0.000813	0.298444
-1.377990	-1.297507	4.111245	0.000807	0.298730
-1.194015	-1.269313	4.121242	0.000773	0.299028
-1.076352	-1.224604	4.131238	0.000751	0.299348
-0.532704	-1.269799	4.141235	0.000650	0.299606
-0.663067	-1.179251	4.151232	0.000674	0.299928
-0.316012	-1.180692	4.161229	0.000610	0.300225
-0.984640	-0.981552	4.171226	0.000734	0.300599
-1.127866	-0.893830	4.181222	0.000761	0.300895
-0.916696	-0.861646	4.191219	0.000722	0.301234
-0.674182	-0.833975	4.201216	0.000677	0.301578
-0.707044	-0.752851	4.211213	0.000683	0.301938
-0.529477	-0.711111	4.221210	0.000650	0.302292
-0.254555	-0.684029	4.231206	0.000599	0.302660
-0.022882	-0.637498	4.241203	0.000556	0.303083
0.078861	-0.585413	4.251200	0.000537	0.303419
-0.013008	-0.489773	4.261197	0.000554	0.303795
-0.140182	-0.384610	4.271194	0.000578	0.304185
-0.329452	-0.257567	4.281190	0.000613	0.304625
-0.182218	-0.192727	4.291187	0.000585	0.305060
0.199812	-0.174979	4.301184	0.000514	0.305473
0.309774	-0.106477	4.311181	0.000494	0.305891
0.627684	-0.081424	4.321178	0.000435	0.306282
0.471729	0.040004	4.331174	0.000464	0.306721
0.000000	0.225519	4.341171	0.000552	0.307191

0.258467	0.451637	4.346176	0.000503	0.308475
0.416333	0.973322	4.351181	0.000474	0.311045
0.292382	1.839857	4.356186	0.000496	0.314947
0.803737	2.866390	4.361190	0.000400	0.320048
1.678920	4.119442	4.366195	0.000237	0.326369
1.909914	5.793397	4.371200	0.000193	0.333890
2.255705	7.736059	4.376205	0.000127	0.342470
2.990578	9.926421	4.381210	-0.000011	0.352150
2.923627	12.567127	4.386214	-0.000000	0.362789
3.582347	15.388272	4.391219	-0.000125	0.374333
4.023550	18.583439	4.396224	-0.000209	0.386785
4.408448	22.118623	4.401229	-0.000283	0.400042
5.210635	25.921143	4.406234	-0.000435	0.414073
5.407900	30.182614	4.411238	-0.000474	0.428825
6.020215	34.705193	4.416243	-0.000591	0.444182
6.850618	39.544108	4.421248	-0.000749	0.460145
7.148634	44.829471	4.426253	-0.000808	0.476636
7.657500	50.423766	4.431258	-0.000906	0.493593
8.463879	56.306887	4.436262	-0.001060	0.510957
8.643393	62.636817	4.441267	-0.001098	0.528663
9.376752	69.185782	4.446272	-0.001238	0.546640
9.301957	76.189554	4.451277	-0.001229	0.564836
9.814211	83.391033	4.456282	-0.001329	0.583216
10.530622	90.824194	4.461286	-0.001467	0.601680
11.059003	98.569488	4.466291	-0.001571	0.620243
11.677302	106.552850	4.471296	-0.001691	0.638842
12.453488	114.733816	4.476301	-0.001841	0.657410
12.801592	123.214483	4.481306	-0.001911	0.675946
13.805093	131.743839	4.486310	-0.002103	0.694332
17.937195	139.933819	4.491315	-0.002878	0.712685
20.172749	148.677082	4.496320	-0.003300	0.731001
20.777344	157.847450	4.501325	-0.003418	0.749132
21.979550	167.023224	4.506330	-0.003648	0.767044
22.037397	176.517972	4.511334	-0.003665	0.784760
22.726411	185.965043	4.516339	-0.003800	0.802200
24.280166	195.333306	4.521344	-0.004095	0.819399
25.126670	204.894797	4.526349	-0.004259	0.836362
26.050409	214.463190	4.531354	-0.004437	0.853021
27.043963	224.045606	4.536358	-0.004628	0.869404
28.103097	233.635798	4.541363	-0.004832	0.885515
29.756006	243.140895	4.546368	-0.005145	0.901368
31.253564	252.670788	4.551373	-0.005430	0.916942
32.716761	262.201077	4.556378	-0.005709	0.932246
33.735240	271.802962	4.561382	-0.005905	0.947292
34.549488	281.416749	4.566387	-0.006063	0.962066
35.559291	290.956007	4.571392	-0.006257	0.976556
35.966927	300.573641	4.576397	-0.006339	0.990795
37.414965	309.942387	4.581402	-0.006615	1.004735
38.233148	319.380526	4.586406	-0.006773	1.018425
38.447942	328.886430	4.591411	-0.006819	1.031882
39.430183	338.187017	4.596416	-0.007008	1.045066
40.430512	347.429771	4.601421	-0.007201	1.058009
41.420457	356.675455	4.606426	-0.007391	1.070798
41.621690	365.978546	4.611430	-0.007434	1.083329
42.562624	375.087719	4.616435	-0.007615	1.095630
43.007092	384.254964	4.621440	-0.007704	1.107758
44.361674	393.191335	4.626445	-0.007962	1.119658
45.881970	402.096699	4.631450	-0.008251	1.131429
46.780177	411.081720	4.636454	-0.008424	1.143043
47.632959	420.054605	4.641459	-0.008589	1.154516
48.282374	428.981360	4.646464	-0.008715	1.165774
49.126954	437.831180	4.651469	-0.008878	1.176871
49.984910	446.658194	4.656474	-0.009044	1.187839
49.763101	455.633311	4.661478	-0.009008	1.198663
50.362891	464.406116	4.666483	-0.009126	1.209316
51.169395	473.125962	4.671488	-0.009281	1.219854
51.984754	481.806613	4.676493	-0.009439	1.230257
52.589038	490.506529	4.681498	-0.009557	1.240553
53.609792	499.087828	4.686502	-0.009753	1.250708
53.882439	507.792920	4.691507	-0.009809	1.260778
54.214300	516.475594	4.696512	-0.009876	1.270754
55.049559	524.985281	4.701517	-0.010037	1.280553
55.372299	533.612931	4.706522	-0.010103	1.290312
55.215516	542.288177	4.711526	-0.010080	1.299961
55.864776	550.808261	4.716531	-0.010206	1.309518
56.473504	559.355248	4.721536	-0.010325	1.319027
57.216963	567.751016	4.726541	-0.010469	1.328327
57.568404	576.258937	4.731546	-0.010540	1.337613
58.321842	584.647800	4.736550	-0.010685	1.346779
58.755372	593.106130	4.741555	-0.010771	1.355900
59.701254	601.451000	4.746560	-0.010953	1.364930
60.612350	609.799873	4.751565	-0.011128	1.373898
61.431906	618.173734	4.756570	-0.011286	1.382818
61.781731	626.636196	4.761574	-0.011357	1.391692
61.949608	635.068989	4.766579	-0.011393	1.400447
62.379422	643.458619	4.771584	-0.011479	1.409148
62.672117	651.847428	4.776589	-0.011539	1.417771
63.342952	660.172690	4.781594	-0.011669	1.426342
63.494194	668.591882	4.786598	-0.011703	1.434868
64.393743	676.845422	4.791603	-0.011875	1.443303
65.040116	685.161160	4.796608	-0.012001	1.451708
65.400134	693.514554	4.801613	-0.012074	1.460055
66.438810	701.792151	4.806618	-0.012272	1.468390
67.029638	710.105372	4.811622	-0.012388	1.476640
67.155477	718.458354	4.816627	-0.012417	1.484809
67.361311	726.823022	4.821632	-0.012460	1.492956
67.965497	735.054816	4.826637	-0.012578	1.500995
68.519036	743.349991	4.831642	-0.012687	1.509043
69.078480	751.612223	4.836646	-0.012796	1.517018
69.414959	759.907623	4.841651	-0.012864	1.524947
69.649646	768.230486	4.846656	-0.012913	1.532846
70.601704	776.365706	4.851661	-0.013096	1.540638
71.392496	784.608218	4.856666	-0.013248	1.548466
71.839735	792.875236	4.861670	-0.013337	1.556225
72.050479	801.162121	4.866675	-0.013382	1.563928
72.394670	809.462129	4.871680	-0.013451	1.571626
72.555303	817.735699	4.876685	-0.013486	1.579234
72.849585	825.996627	4.881690	-0.013546	1.586814
73.666806	834.139535	4.886694	-0.013704	1.594328
73.691783	842.432359	4.891699	-0.013714	1.601825
74.605041	850.586419	4.896704	-0.013889	1.609292
74.748724	858.870976	4.901709	-0.013921	1.616730
75.560939	867.020253	4.906714	-0.014078	1.624109
75.574181	875.346049	4.911718	-0.014086	1.631497
75.925484	883.552792	4.916723	-0.014156	1.638795
76.648341	891.683773	4.921728	-0.014296	1.646046
76.730991	899.956562	4.926733	-0.014317	1.653299
77.481964	908.085994	4.931738	-0.014462	1.660489
77.913303	916.294699	4.936742	-0.014548	1.667672
78.063930	924.537630	4.941747	-0.014581	1.674815
79.021879	932.623499	4.946752	-0.014765	1.681903
78.821573	940.926362	4.951757	-0.014733	1.688989
79.878912	949.002799	4.956762	-0.014935	1.696023
79.908446	957.282897	4.961766	-0.014946	1.703061
79.626569	965.573543	4.966771	-0.014898	1.710039
79.587230	973.828506	4.971776	-0.014896	1.716990
80.879185	981.785831	4.976781	-0.015142	1.723839
81.369228	989.955060	4.981786	-0.015239	1.730733
82.004683	998.106166	4.986790	-0.015362	1.737603
81.859178	1006.391988	4.991795	-0.015341	1.744456
82.301694	1014.575417	4.996800	-0.015428	1.751273
82.582142	1022.750478	5.001805	-0.015486	1.758036
83.130464	1030.884124	5.006810	-0.015593	1.764774
84.061134	1038.966112	5.011814	-0.015772	1.771492
84.225345	1047.175372	5.016819	-0.015807	1.778191
84.794395	1055.307510	5.021824	-0.015919	1.784854
85.734033	1063.394713	5.026829	-0.016099	1.791501
86.276168	1071.561121	5.031834	-0.016205	1.798138
86.566372	1079.722269	5.036838	-0.016264	1.804715
86.981081	1087.912010	5.041843	-0.016347	1.811305
87.640711	1096.042377	5.046848	-0.016475	1.817855
87.784117	1104.230332	5.051853	-0.016507	1.824364
88.750875	1112.297499	5.056858	-0.016692	1.830854
89.111223	1120.468558	5.061862	-0.016765	1.837329
89.369736	1128.615928	5.066867	-0.016818	1.843751
89.852972	1136.806199	5.071872	-0.016913	1.850210
90.479178	1144.891972	5.076877	-0.017035	1.856583
90.518207	1153.122080	5.081882	-0.017048	1.862976
90.541934	1161.343453	5.086886	-0.017057	1.869338
91.072808	1169.430033	5.091891	-0.017162	1.875635
92.073712	1177.453077	5.096896	-0.017353	1.881917
91.569680	1185.734153	5.101901	-0.017265	1.888199
92.255000	1193.809522	5.106906	-0.017397	1.894442
92.816001	1201.909533	5.111910	-0.017507	1.900669
93.277860	1210.028626	5.116915	-0.017598	1.906878
93.487144	1218.238451	5.121920	-0.017643	1.913106
94.319441	1226.258235	5.126925	-0.017803	1.919243
94.900801	1234.368506	5.131930	-0.017916	1.925399
95.023515	1242.571980	5.136934	-0.017944	1.931552
95.447269	1250.687087	5.141939	-0.018029	1.937655
96.606233	1258.697629	5.146944	-0.018250	1.943742
97.217110	1266.802825	5.151949	-0.018369	1.949820
97.326171	1274.999903	5.156954	-0.018394	1.955890
97.370092	1283.175917	5.161958	-0.018408	1.961919
97.333010	1291.332265	5.166963	-0.018406	1.967906
97.853585	1299.432795	5.171968	-0.018508	1.973895
97.921468	1307.573951	5.176973	-0.018526	1.979846
98.340772	1315.691839	5.181978	-0.018609	1.985800
98.720584	1323.784790	5.186982	-0.018685	1.991714
98.989038	1331.904491	5.191987	-0.018741	1.997618
99.792828	1339.928823	5.196992	-0.018895	2.003493
99.822555	1348.103013	5.201997	-0.018906	2.009376
99.870112	1356.274795	5.207002	-0.018920	2.015242
100.636914	1364.315177	5.212006	-0.019068	2.021073
101.005663	1372.409923	5.217011	-0.019142	2.026883
100.847699	1380.636525	5.222016	-0.019118	2.032715
100.548643	1388.816654	5.227021	-0.019068	2.038483
101.315424	1396.787875	5.232026	-0.019216	2.044199
101.701613	1404.877841	5.237030	-0.019293	2.049942
102.243693	1412.936300	5.242035	-0.019399	2.055663
102.994721	1420.979139	5.247040	-0.019544	2.061379
102.843397	1429.181666	5.252045	-0.019521	2.067097
103.442444	1437.261348	5.257050	-0.019638	2.072791
103.644077	1445.383493	5.262054	-0.019681	2.078458
104.165072	1453.440701	5.267059	-0.019783	2.084097
104.687806	1461.510186	5.272064	-0.019885	2.089730
104.772099	1469.670806	5.277069	-0.019906	2.095366
105.526961	1477.699674	5.282074	-0.020052	2.100963
105.752981	1485.832499	5.287078	-0.020099	2.106564
106.070191	1493.965005	5.292083	-0.020164	2.112158
106.174739	1502.135754	5.297088	-0.020189	2.117743
106.356212	1510.218713	5.302093	-0.020228	2.123261
106.747882	1518.280933	5.307098	-0.020306	2.128771
107.287204	1526.328251	5.312102	-0.020411	2.134271
107.529438	1534.405590	5.317107	-0.020462	2.139749
107.944312	1542.501699	5.322112	-0.020544	2.145241
108.071888	1550.625790	5.327117	-0.020573	2.150711
108.850404	1558.646354	5.332122	-0.020723	2.156159
109.305940	1566.721292	5.337126	-0.020813	2.161600
109.604529	1574.842706	5.342131	-0.020874	2.167042
110.715434	1582.820592	5.347136	-0.021086	2.172453
111.300593	1590.884211	5.352141	-0.021200	2.177857
111.782433	1598.981402	5.357146	-0.021295	2.183259
111.800481	1607.183826	5.362150	-0.021304	2.188674
112.285221	1615.253295	5.367155	-0.021399	2.194032
112.630234	1623.352249	5.372160	-0.021469	2.199384
113.061286	1631.395771	5.377165	-0.021554	2.204693
113.783216	1639.441708	5.382170	-0.021694	2.210019
114.046593	1647.580161	5.387174	-0.021748	2.215349
113.835036	1655.757485	5.392179	-0.021714	2.220648
114.846571	1663.720656	5.397184	-0.021908	2.225908
114.975242	1671.851975	5.402189	-0.021937	2.231183
114.844983	1680.003753	5.407194	-0.021918	2.236435
115.134214	1688.083642	5.412198	-0.021977	2.241667
115.358544	1696.161833	5.417203	-0.022024	2.246880
115.506118	1704.281657	5.422208	-0.022057	2.252100
116.149090	1712.291023	5.427213	-0.022182	2.257282
116.993819	1720.295722	5.432218	-0.022344	2.262467
117.573222	1728.370170	5.437222	-0.022457	2.267661
117.656692	1736.550869	5.442227	-0.022478	2.272866
118.244638	1744.602292	5.447232	-0.022593	2.278022
118.610750	1752.644158	5.452237	-0.022666	2.283140
118.581409	1760.776552	5.457242	-0.022666	2.288270
118.559973	1768.901272	5.462246	-0.022667	2.293383
118.870697	1776.950154	5.467251	-0.022730	2.298467
119.725238	1784.917262	5.472256	-0.022894	2.303535
120.335928	1792.958158	5.477261	-0.023013	2.308617
120.694447	1801.073492	5.482266	-0.023085	2.313713
120.955842	1809.153336	5.487270	-0.023139	2.318767
121.382582	1817.186283	5.492275	-0.023224	2.323794
122.047758	1825.247826	5.497280	-0.023353	2.328849
122.740860	1833.298524	5.502285	-0.023487	2.333888
122.846014	1841.444001	5.507290	-0.023512	2.338925
123.092758	1849.544652	5.512294	-0.023563	2.343936
123.211297	1857.660985	5.517299	-0.023590	2.348934
123.787463	1865.718862	5.522304	-0.023703	2.353925
124.022672	1873.765555	5.527309	-0.023752	2.358869
124.454701	1881.799245	5.532314	-0.023838	2.363812
124.646259	1889.903178	5.537318	-0.023879	2.368767
125.018110	1897.959723	5.542323	-0.023953	2.373697
125.285253	1906.062890	5.547328	-0.024008	2.378637
125.256428	1914.159850	5.552333	-0.024008	2.383539
126.051936	1922.144220	5.557338	-0.024161	2.388430
126.195332	1930.262057	5.562342	-0.024193	2.393338
126.557311	1938.279795	5.567347	-0.024266	2.398193
127.210834	1946.309749	5.572352	-0.024392	2.403070
127.295588	1954.411855	5.577357	-0.024414	2.407933
127.529086	1962.516768	5.582362	-0.024462	2.412801
128.370572	1970.519524	5.587366	-0.024624	2.417646
128.402267	1978.623644	5.592371	-0.024635	2.422478
128.863280	1986.703839	5.597376	-0.024726	2.427320
128.993706	1994.829730	5.602381	-0.024756	2.432152
129.456248	2002.880792	5.607386	-0.024847	2.436957
129.731597	2010.918708	5.612390	-0.024904	2.441731
130.475717	2018.876534	5.617395	-0.025047	2.446484
130.773789	2026.997971	5.622400	-0.025108	2.451289
130.916331	2035.094142	5.627405	-0.025140	2.456058
131.592008	2043.108125	5.632410	-0.025271	2.460810
131.769250	2051.196755	5.637414	-0.025309	2.465559
132.276735	2059.210338	5.642419	-0.025409	2.470280
132.925923	2067.251527	5.647424	-0.025535	2.475019
133.167719	2075.343446	5.652429	-0.025585	2.479747
133.969347	2083.319314	5.657434	-0.025739	2.484441
134.129370	2091.469580	5.662438	-0.025775	2.489178
134.346351	2099.544350	5.667443	-0.025820	2.493867
134.596694	2107.645808	5.672448	-0.025872	2.498565
134.913759	2115.673778	5.677453	-0.025936	2.503217
135.179240	2123.746404	5.682458	-0.025991	2.507882
135.668136	2131.805526	5.687462	-0.026087	2.512548
136.189218	2139.800554	5.692467	-0.026189	2.517170
136.448497	2147.904823	5.697472	-0.026243	2.521826
136.762686	2155.935087	5.702477	-0.026307	2.526436
136.923280	2164.041962	5.707482	-0.026342	2.531070
137.378495	2172.075625	5.712486	-0.026432	2.535675
137.639522	2180.133474	5.717491	-0.026485	2.540271
137.776930	2188.232981	5.722496	-0.026516	2.544874
138.295714	2196.237355	5.727501	-0.026618	2.549442
138.555477	2204.345430	5.732506	-0.026672	2.554041
139.284583	2212.322988	5.737510	-0.026813	2.558592
139.629168	2220.355111	5.742515	-0.026882	2.563139
139.743573	2228.499716	5.747520	-0.026908	2.567724
139.778332	2236.593048	5.752525	-0.026920	2.572266
140.291662	2244.617338	5.757530	-0.027021	2.576795
140.252261	2252.745726	5.762534	-0.027019	2.581336
140.733448	2260.716936	5.767539	-0.027114	2.585817
141.247909	2268.788392	5.772544	-0.027215	2.590349
141.232975	2276.977657	5.777549	-0.027217	2.594901
141.946122	2284.896450	5.782554	-0.027355	2.599347
142.033684	2292.978162	5.787558	-0.027377	2.603831
142.271962	2301.004938	5.792563	-0.027426	2.608287
142.932466	2309.009045	5.797568	-0.027554	2.612752
143.041289	2317.102013	5.802573	-0.027580	2.617221
143.705178	2325.096894	5.807578	-0.027709	2.621666
144.022607	2333.163228	5.812582	-0.027773	2.626119
144.349888	2341.206615	5.817587	-0.027839	2.630552
144.664285	2349.293061	5.822592	-0.027903	2.635001
144.887254	2357.318690	5.827597	-0.027949	2.639402
145.102311	2365.374302	5.832602	-0.027995	2.643812
145.872291	2373.369029	5.837606	-0.028143	2.648219
145.719184	2381.521578	5.842611	-0.028120	2.652642
146.264482	2389.540123	5.847616	-0.028227	2.657032
146.343806	2397.610683	5.852621	-0.028247	2.661412
146.934608	2405.618934	5.857626	-0.028362	2.665784
147.050814	2413.735454	5.862630	-0.028389	2.670177
147.339385	2421.760843	5.867635	-0.028448	2.674524
147.947564	2429.748131	5.872640	-0.028566	2.678865
148.372682	2437.754275	5.877645	-0.028650	2.683197
148.172118	2445.917547	5.882650	-0.028618	2.687565
149.119562	2453.864818	5.887654	-0.028800	2.691885
149.557458	2461.921317	5.892659	-0.028887	2.696223
149.804346	2470.014268	5.897664	-0.028938	2.700562
149.996058	2478.047976	5.902669	-0.028979	2.704858
149.660596	2486.227097	5.907674	-0.028922	2.709191
150.023949	2494.256435	5.912678	-0.028994	2.713482
150.609813	2502.193534	5.917683	-0.029109	2.717731
151.249068	2510.224240	5.922688	-0.029233	2.722027
151.241063	2518.308698	5.927693	-0.029237	2.726303
151.703487	2526.359980	5.932698	-0.029328	2.730585
152.438791	2534.355301	5.937702	-0.029470	2.734848
153.175048	2542.333153	5.942707	-0.029612	2.739095
153.176613	2550.475254	5.947712	-0.029618	2.743375
153.458450	2558.515668	5.952717	-0.029675	2.747613
153.937880	2566.584469	5.957722	-0.029770	2.751871
154.308574	2574.649730	5.962726	-0.029844	2.756115
154.218834	2582.736878	5.967731	-0.029833	2.760334
154.809937	2590.722679	5.972736	-0.029948	2.764536
154.989959	2598.769042	5.977741	-0.029987	2.768738
155.127824	2606.857954	5.982746	-0.030018	2.772953
155.530009	2614.885352	5.987750	-0.030098	2.777146
155.867068	2622.900851	5.992755	-0.030166	2.781322
155.949370	2630.988734	5.997760	-0.030186	2.785514
155.330258	2639.156700	6.002765	-0.030076	2.789699
155.820393	2647.138770	6.007770	-0.030173	2.793848
156.500453	2655.090760	6.012774	-0.030304	2.797987
157.200349	2663.048955	6.017779	-0.030440	2.802124
157.379435	2671.164576	6.022784	-0.030478	2.806305
157.633791	2679.219702	6.027789	-0.030531	2.810453
157.727408	2687.319590	6.032794	-0.030554	2.814608
158.485817	2695.274355	6.037798	-0.030700	2.818722
158.651361	2703.329428	6.042803	-0.030736	2.822846
159.179729	2711.368511	6.047808	-0.030840	2.826978
159.213610	2719.465705	6.052813	-0.030851	2.831103
159.685979	2727.493481	6.057818	-0.030944	2.835214
160.005079	2735.508975	6.062822	-0.031009	2.839302
160.041159	2743.539143	6.067827	-0.031021	2.843376
160.544231	2751.567411	6.072832	-0.031120	2.847471
160.867974	2759.629905	6.077837	-0.031185	2.851566
160.525035	2767.800786	6.082842	-0.031126	2.855671
161.350587	2775.726614	6.087846	-0.031285	2.859714
161.536646	2783.766121	6.092851	-0.031325	2.863772
161.408862	2791.918079	6.097856	-0.031307	2.867863
161.524332	2799.949448	6.102861	-0.031333	2.871902
161.992831	2807.945337	6.107866	-0.031426	2.875936
162.348380	2815.958630	6.112870	-0.031497	2.879968
162.115216	2824.046079	6.117875	-0.031459	2.883997
162.576491	2832.047666	6.122880	-0.031550	2.888018
162.911556	2840.089905	6.127885	-0.031618	2.892045
163.927726	2848.019968	6.132890	-0.031812	2.896050
164.163046	2856.105692	6.137894	-0.031861	2.900082
164.751504	2864.087753	6.142899	-0.031976	2.904077
165.304878	2872.149339	6.147904	-0.032084	2.908104
165.295450	2880.307277	6.152909	-0.032087	2.912141
165.411818	2888.407547	6.157914	-0.032114	2.916152
165.674982	2896.431207	6.162918	-0.032169	2.920127
166.148250	2904.355816	6.167923	-0.032262	2.924060
166.274482	2912.456079	6.172928	-0.032291	2.928054
166.731853	2920.450162	6.177933	-0.032381	2.932009
166.924733	2928.516937	6.182938	-0.032422	2.935980
167.128330	2936.575723	6.187942	-0.032465	2.939942
167.523749	2944.567614	6.192947	-0.032544	2.943876
168.128043	2952.583264	6.197952	-0.032662	2.947828
167.799234	2960.740412	6.202957	-0.032606	2.951794
167.911088	2968.801855	6.207962	-0.032632	2.955731
167.871356	2976.838066	6.212966	-0.032629	2.959643
167.816616	2984.846706	6.217971	-0.032624	2.963535
168.570587	2992.793291	6.222976	-0.032770	2.967434
168.521435	3000.919764	6.227981	-0.032766	2.971374
168.904743	3008.924988	6.232986	-0.032843	2.975272
169.008269	3016.974431	6.237990	-0.032867	2.979172
169.532714	3024.944397	6.242995	-0.032970	2.983050
170.633496	3032.899126	6.248000	-0.033180	2.986945
170.435213	3041.084404	6.253005	-0.033148	2.990879
170.770404	3049.098407	6.258010	-0.033216	2.994754
171.429797	3057.083002	6.263014	-0.033344	2.998625
171.689785	3065.070915	6.268019	-0.033397	3.002473
171.987342	3073.163607	6.273024	-0.033458	3.006367
172.330816	3081.194851	6.278029	-0.033527	3.010230
172.183163	3089.327435	6.283034	-0.033505	3.014111
172.405270	3097.359828	6.288038	-0.033552	3.017958
172.845704	3105.349957	6.293043	-0.033639	3.021791
172.951395	3113.409523	6.298048	-0.033664	3.025635
172.532317	3121.511221	6.303053	-0.033591	3.029468
172.766152	3129.546200	6.308058	-0.033640	3.033297
173.695425	3137.482682	6.313062	-0.033818	3.037109
174.058308	3145.489156	6.318067	-0.033890	3.040921
174.472343	3153.521630	6.323072	-0.033973	3.044744
174.977872	3161.529067	6.328077	-0.034072	3.048554
175.238227	3169.636603	6.333082	-0.034126	3.052394
175.282571	3177.738599	6.338086	-0.034139	3.056216
175.680271	3185.692576	6.343091	-0.034218	3.059982
176.487769	3193.664454	6.348096	-0.034374	3.063770
176.358962	3201.794293	6.353101	-0.034355	3.067583
176.554411	3209.838023	6.358106	-0.034397	3.071366
176.945501	3217.925564	6.363110	-0.034475	3.075175
177.090420	3225.911224	6.368115	-0.034507	3.078919
177.453539	3233.924991	6.373120	-0.034580	3.082682
176.876311	3242.072805	6.378125	-0.034478	3.086458
177.341866	3250.056361	6.383130	-0.034569	3.090203
177.339403	3258.129285	6.388134	-0.034574	3.093963
177.960158	3266.022769	6.393139	-0.034695	3.097664
178.314901	3274.101747	6.398144	-0.034766	3.101434
178.650843	3282.080903	6.403149	-0.034834	3.105152
178.707291	3290.160206	6.408154	-0.034850	3.108899
179.050542	3298.228987	6.413158	-0.034919	3.112650
179.458624	3306.207204	6.418163	-0.035000	3.116358
179.849647	3314.231362	6.423168	-0.035078	3.120082
179.850210	3322.259294	6.428173	-0.035083	3.123784
180.528698	3330.271272	6.433178	-0.035215	3.127507
180.930789	3338.348062	6.438182	-0.035295	3.131242
180.862040	3346.392168	6.443187	-0.035287	3.134935
181.500919	3354.406940	6.448192	-0.035411	3.138644
181.524896	3362.482005	6.453197	-0.035421	3.142347
181.476993	3370.554677	6.458202	-0.035417	3.146041
181.888818	3378.548764	6.463206	-0.035499	3.149717
182.259667	3386.535957	6.468211	-0.035573	3.153383
182.332338	3394.624466	6.473216	-0.035592	3.157077
182.741500	3402.608359	6.478221	-0.035673	3.160734
182.811119	3410.637269	6.483226	-0.035692	3.164393
183.406485	3418.658780	6.488230	-0.035808	3.168067
183.551719	3426.730707	6.493235	-0.035840	3.171740
183.971972	3434.783033	6.498240	-0.035923	3.175411
183.726607	3442.853518	6.503245	-0.035883	3.179058
184.167070	3450.824060	6.508250	-0.035970	3.182685
184.591430	3458.855932	6.513254	-0.036054	3.186335
184.673786	3466.913213	6.518259	-0.036075	3.189977
184.802237	3474.989819	6.523264	-0.036104	3.193625
184.997736	3482.989503	6.528269	-0.036145	3.197238
185.466102	3490.985834	6.533274	-0.036238	3.200857
185.516272	3499.035985	6.538278	-0.036252	3.204478
185.747685	3507.044424	6.543283	-0.036301	3.208084
186.767427	3515.020349	6.548288	-0.036496	3.211705
186.934991	3523.089629	6.553293	-0.036532	3.215327
187.056768	3531.141766	6.558298	-0.036560	3.218936
187.268793	3539.172720	6.563302	-0.036605	3.222535
187.397502	3547.246593	6.568307	-0.036634	3.226145
187.776260	3555.245555	6.573312	-0.036710	3.229728
187.794738	3563.346003	6.578317	-0.036718	3.233338
188.356143	3571.265080	6.583322	-0.036828	3.236885
188.916614	3579.301444	6.588326	-0.036937	3.240481
189.474831	3587.214258	6.593331	-0.037046	3.244017
189.741456	3595.338122	6.598336	-0.037101	3.247631
190.011232	3603.389084	6.603341	-0.037157	3.251209
190.281023	3611.413052	6.608346	-0.037212	3.254771
190.797519	3619.453252	6.613350	-0.037314	3.258346
191.359981	3627.429628	6.618355	-0.037423	3.261891
191.547317	3635.538452	6.623360	-0.037464	3.265476
191.822159	3643.533994	6.628365	-0.037520	3.269009
192.103414	3651.590968	6.633370	-0.037578	3.272567
191.960821	3659.707472	6.638374	-0.037556	3.276129
192.029848	3667.669501	6.643379	-0.037574	3.279628
192.380936	3675.707349	6.648384	-0.037645	3.283168
192.526919	3683.752251	6.653389	-0.037677	3.286699
192.594308	3691.819523	6.658394	-0.037695	3.290233
192.911989	3699.854713	6.663398	-0.037759	3.293759
193.385287	3707.789328	6.668403	-0.037853	3.297243
194.153252	3715.820958	6.673408	-0.038001	3.300778
194.291702	3723.809947	6.678413	-0.038032	3.304265
194.871263	3731.826211	6.683418	-0.038145	3.307778
194.902041	3739.986507	6.688422	-0.038156	3.311328
194.984461	3747.973309	6.693427	-0.038176	3.314801
195.378195	3756.005216	6.698432	-0.038255	3.318302
195.101607	3764.107616	6.703437	-0.038208	3.321804
195.512752	3772.052764	6.708442	-0.038290	3.325260
196.066251	3780.060049	6.713446	-0.038398	3.328746
196.114811	3788.124797	6.718451	-0.038413	3.332233
196.381238	3796.193043	6.723456	-0.038467	3.335726
196.540063	3804.176610	6.728461	-0.038502	3.339175
196.870013	3812.194633	6.733466	-0.038569	3.342641
197.696263	3820.172045	6.738470	-0.038728	3.346106
197.302676	3828.311138	6.743475	-0.038660	3.349590
197.995809	3836.281819	6.748480	-0.038794	3.353039
198.440485	3844.302599	6.753485	-0.038882	3.356497
198.513034	3852.328869	6.758490	-0.038901	3.359939
198.809403	3860.367858	6.763494	-0.038961	3.363392
198.782558	3868.423094	6.768499	-0.038961	3.366835
199.177680	3876.473849	6.773504	-0.039040	3.370290
199.394306	3884.462982	6.778509	-0.039086	3.373707
199.442872	3892.533548	6.783514	-0.039100	3.377150
199.680277	3900.581331	6.788518	-0.039149	3.380586
200.294408	3908.462394	6.793523	-0.039269	3.383962
200.514525	3916.562022	6.798528	-0.039315	3.387413
200.711655	3924.634485	6.803533	-0.039357	3.390848
200.575875	3932.698196	6.808538	-0.039337	3.394263
201.465964	3940.647339	6.813542	-0.039508	3.397664
201.456062	3948.708456	6.818547	-0.039511	3.401076
202.189044	3956.626347	6.823552	-0.039653	3.404451
202.224015	3964.737600	6.828557	-0.039664	3.407879
202.134658	3972.838746	6.833562	-0.039653	3.411295
202.484000	3980.836692	6.838566	-0.039723	3.414679
202.868480	3988.795278	6.843571	-0.039800	3.418045
202.757156	3996.911382	6.848576	-0.039784	3.421456
203.085271	4004.877415	6.853581	-0.039851	3.424816
203.413191	4012.913928	6.858586	-0.039917	3.428203
203.799929	4020.953621	6.863590	-0.039994	3.431589
204.014637	4028.951736	6.868595	-0.040039	3.434949
204.381792	4036.987594	6.873600	-0.040113	3.438326
204.695073	4044.985238	6.878605	-0.040176	3.441682
204.537740	4053.087478	6.883610	-0.040152	3.445063
204.602093	4061.157544	6.888614	-0.040169	3.448434
204.965823	4069.123924	6.893619	-0.040242	3.451769
205.136073	4077.181609	6.898624	-0.040279	3.455132
205.447294	4085.195114	6.903629	-0.040342	3.458478
206.127584	4093.186247	6.908634	-0.040474	3.461824
206.516581	4101.164171	6.913638	-0.040552	3.465151
206.887298	4109.196602	6.918643	-0.040626	3.468498
207.321434	4117.242352	6.923648	-0.040712	3.471848
207.339182	4125.292977	6.928653	-0.040721	3.475183
207.723536	4133.287659	6.933658	-0.040797	3.478504
207.975894	4141.367333	6.938662	-0.040849	3.481853
208.274606	4149.339242	6.943667	-0.040910	3.485156
208.603607	4157.381521	6.948672	-0.040977	3.488485
208.541747	4165.444845	6.953677	-0.040970	3.491807
209.357283	4173.403068	6.958682	-0.041127	3.495111
209.583393	4181.489191	6.963686	-0.041175	3.498445
209.824540	4189.470996	6.968691	-0.041225	3.501734
209.561011	4197.622256	6.973696	-0.041181	3.505073
209.884182	4205.578555	6.978701	-0.041246	3.508347
210.182989	4213.602289	6.983706	-0.041307	3.511646
210.398031	4221.635747	6.988710	-0.041352	3.514942
210.137983	4229.709682	6.993715	-0.041309	3.518237
210.691314	4237.693558	6.998720	-0.041417	3.521518
210.676687	4245.712815	7.003725	-0.041420	3.524792
211.070513	4253.718323	7.008730	-0.041498	3.528070
211.762756	4261.737324	7.013734	-0.041632	3.531361
211.674957	4269.778766	7.018739	-0.041621	3.534632
212.754161	4277.704852	7.023744	-0.041827	3.537891
212.732183	4285.803112	7.028749	-0.041828	3.541181
212.895811	4293.806884	7.033754	-0.041864	3.544436
213.230948	4301.877266	7.038758	-0.041932	3.547721
213.775282	4309.894527	7.043763	-0.042038	3.550987
213.739426	4318.009378	7.048768	-0.042037	3.554271
213.618323	4326.056395	7.053773	-0.042019	3.557523
214.442636	4333.962175	7.058778	-0.042178	3.560744
215.034578	4341.891611	7.063782	-0.042293	3.563964
215.091308	4349.987529	7.068787	-0.042309	3.567231
215.735341	4357.996898	7.073792	-0.042434	3.570479
215.913907	4366.059051	7.078797	-0.042473	3.573731
216.281789	4374.074025	7.083802	-0.042546	3.576967
216.305489	4382.153337	7.088806	-0.042556	3.580215
216.532858	4390.111985	7.093811	-0.042604	3.583418
216.807935	4398.205089	7.098816	-0.042660	3.586673
216.706334	4406.252682	7.103821	-0.042646	3.589896
217.374053	4414.171578	7.108826	-0.042776	3.593087
217.442562	4422.292854	7.113830	-0.042794	3.596339
217.149764	4430.318507	7.118835	-0.042744	3.599539
217.725815	4438.278569	7.123840	-0.042857	3.602735
218.040023	4446.310603	7.128845	-0.042920	3.605949
217.927870	4454.349076	7.133850	-0.042905	3.609151
217.742455	4462.495657	7.138854	-0.042876	3.612391
218.280408	4470.408399	7.143859	-0.042981	3.615555
218.752046	4478.428189	7.148864	-0.043074	3.618758
218.941965	4486.457645	7.153869	-0.043114	3.621953
219.677949	4494.416247	7.158874	-0.043257	3.625133
219.579187	4502.562081	7.163878	-0.043243	3.628361
220.030318	4510.516352	7.168883	-0.043333	3.631525
220.526792	4518.491089	7.173888	-0.043430	3.634696
220.125989	4526.633535	7.178893	-0.043361	3.637906
220.708111	4534.576944	7.183898	-0.043474	3.641061
221.116092	4542.550182	7.188902	-0.043555	3.644220
220.732113	4550.691222	7.193907	-0.043489	3.647421
221.452875	4558.657286	7.198912	-0.043629	3.650581
221.478613	4566.693095	7.203917	-0.043639	3.653746
221.808609	4574.716869	7.208922	-0.043705	3.656912
222.620933	4582.690874	7.213926	-0.043862	3.660069
222.914316	4590.620963	7.218931	-0.043921	3.663192
222.814042	4598.783606	7.223936	-0.043908	3.666392
223.208308	4606.805818	7.228941	-0.043987	3.669548
223.373838	4614.857367	7.233946	-0.044023	3.672706
223.655452	4622.901515	7.238950	-0.044080	3.675863
223.993782	4630.856947	7.243955	-0.044148	3.678983
224.238375	4638.916868	7.248960	-0.044199	3.682138
224.318286	4646.931909	7.253965	-0.044219	3.685269
224.420728	4654.946664	7.258970	-0.044243	3.688398
224.791831	4662.999643	7.263974	-0.044318	3.691547
224.973666	4670.981099	7.268979	-0.044357	3.694659
225.142944	4679.032042	7.273984	-0.044393	3.697796
225.311562	4687.077092	7.278989	-0.044430	3.700928
225.671336	4695.021257	7.283994	-0.044502	3.704022
225.632898	4703.166414	7.288998	-0.044500	3.707182
225.288952	4711.269712	7.294003	-0.044441	3.710315
225.594255	4719.282302	7.299008	-0.044503	3.713427
225.893809	4727.268250	7.304013	-0.044564	3.716526
226.637849	4735.125676	7.309018	-0.044708	3.719584
226.630220	4743.203779	7.314022	-0.044712	3.722705
226.824509	4751.204950	7.319027	-0.044753	3.725800
227.033452	4759.225663	7.324032	-0.044797	3.728899
227.489605	4767.268518	7.329037	-0.044887	3.732011
227.532232	4775.321851	7.334042	-0.044901	3.735113
227.370042	4783.389595	7.339046	-0.044876	3.738214
227.508872	4791.427322	7.344051	-0.044907	3.741308
227.778276	4799.367365	7.349056	-0.044962	3.744365
227.934387	4807.430383	7.354061	-0.044996	3.747464
228.300450	4815.426349	7.359066	-0.045070	3.750540
228.343618	4823.489746	7.364070	-0.045083	3.753631
228.844661	4831.439105	7.369075	-0.045181	3.756687
228.876111	4839.482324	7.374080	-0.045192	3.759765
229.490732	4847.451693	7.379085	-0.045312	3.762826
229.711064	4855.489674	7.384090	-0.045358	3.765902
229.494921	4863.590614	7.389094	-0.045323	3.768988
229.749688	4871.580739	7.394099	-0.045376	3.772041
230.118530	4879.621098	7.399104	-0.045450	3.775113
230.670720	4887.568071	7.404109	-0.045557	3.778152
230.341851	4895.704886	7.409114	-0.045502	3.781239
231.108491	4903.624597	7.414118	-0.045649	3.784268
231.026377	4911.733691	7.419123	-0.045639	3.787345
231.085342	4919.767358	7.424128	-0.045655	3.790395
231.542777	4927.758203	7.429133	-0.045746	3.793436
232.071040	4935.722452	7.434138	-0.045849	3.796465
232.641119	4943.700636	7.439142	-0.045961	3.799499
232.564049	4951.753121	7.444147	-0.045951	3.802543
233.270709	4959.713824	7.449152	-0.046088	3.805568
233.537247	4967.754249	7.454157	-0.046143	3.808610
233.728629	4975.822336	7.459162	-0.046184	3.811659
234.213256	4983.880919	7.464166	-0.046279	3.814708
234.198038	4991.904133	7.469171	-0.046282	3.817730
234.357633	4999.967190	7.474176	-0.046317	3.820769
234.352249	5007.995126	7.479181	-0.046321	3.823788
234.757293	5015.999125	7.484186	-0.046401	3.826805
235.109878	5024.028545	7.489190	-0.046472	3.829828
235.305276	5032.027166	7.494195	-0.046514	3.832834
235.918150	5040.039170	7.499200	-0.046633	3.835851
236.105351	5048.036948	7.504205	-0.046673	3.838851
236.029428	5056.143274	7.509210	-0.046664	3.841884
236.387215	5064.093688	7.514214	-0.046736	3.844866
236.578978	5072.120274	7.519219	-0.046777	3.847870
236.875679	5080.173058	7.524224	-0.046837	3.850883
236.668886	5088.259745	7.529229	-0.046804	3.853896
236.562211	5096.297483	7.534234	-0.046789	3.856891
237.047074	5104.266355	7.539238	-0.046885	3.859870
237.245996	5112.246234	7.544243	-0.046927	3.862845
237.788312	5120.259774	7.549248	-0.047033	3.865838
237.726235	5128.325070	7.554253	-0.047027	3.868834
237.871745	5136.362968	7.559258	-0.047059	3.871823
238.661027	5144.445677	7.564262	-0.047211	3.874839
238.913369	5152.372391	7.569267	-0.047263	3.877783
239.039686	5160.392389	7.574272	-0.047292	3.880758
239.322332	5168.336475	7.579277	-0.047350	3.883705
239.809625	5176.389285	7.584282	-0.047446	3.886694
239.987299	5184.421772	7.589286	-0.047484	3.889667
240.453667	5192.427608	7.594291	-0.047576	3.892634
241.097260	5200.420682	7.599296	-0.047701	3.895598
241.326665	5208.441186	7.604301	-0.047749	3.898560
241.115911	5216.491991	7.609306	-0.047715	3.901523
241.228564	5224.523559	7.614310	-0.047741	3.904483
241.370002	5232.557167	7.619315	-0.047773	3.907442
241.436387	5240.634124	7.624320	-0.047790	3.910413
241.946342	5248.581970	7.629325	-0.047890	3.913344
242.330207	5256.611684	7.634330	-0.047967	3.916299
242.839863	5264.540441	7.639334	-0.048067	3.919218
242.919606	5272.580920	7.644339	-0.048087	3.922167
243.156906	5280.636166	7.649344	-0.048136	3.925122
243.560070	5288.638462	7.654349	-0.048217	3.928059
243.629452	5296.712365	7.659354	-0.048235	3.931014
243.822324	5304.773921	7.664358	-0.048276	3.933963
244.275008	5312.797219	7.669363	-0.048365	3.936902
244.602442	5320.781899	7.674368	-0.048432	3.939822
244.584421	5328.827445	7.679373	-0.048433	3.942756
245.047852	5336.804325	7.684378	-0.048525	3.945671
244.897905	5344.937341	7.689382	-0.048502	3.948629
244.924600	5352.961731	7.694387	-0.048512	3.951549
244.635657	5361.001372	7.699392	-0.048464	3.954467
245.145140	5368.971702	7.704397	-0.048564	3.957372
245.498511	5376.911313	7.709402	-0.048635	3.960261
245.656530	5384.938230	7.714406	-0.048669	3.963175
246.078244	5392.947489	7.719411	-0.048753	3.966086
245.938758	5401.010852	7.724416	-0.048732	3.969005
246.282048	5409.016238	7.729421	-0.048801	3.971908
246.551937	5417.034751	7.734426	-0.048857	3.974813
246.561189	5425.102441	7.739430	-0.048864	3.977729
246.882287	5433.078482	7.744435	-0.048929	3.980616
247.239727	5441.068183	7.749440	-0.049000	3.983505
246.935696	5449.196773	7.754445	-0.048949	3.986431
247.235381	5457.160429	7.759450	-0.049010	3.989306
247.984946	5465.160965	7.764454	-0.049155	3.992200
247.952431	5473.170843	7.769459	-0.049154	3.995082
248.199467	5481.199051	7.774464	-0.049205	3.997973
248.322359	5489.246978	7.779469	-0.049233	4.000867
248.812861	5497.123996	7.784474	-0.049329	4.003703
248.834285	5505.277282	7.789478	-0.049339	4.006629
249.054371	5513.280756	7.794483	-0.049385	4.009502
249.057180	5521.340454	7.799488	-0.049391	4.012390
248.826058	5529.402163	7.804493	-0.049353	4.015272
249.343938	5537.316562	7.809498	-0.049454	4.018112
249.435466	5545.380769	7.814502	-0.049477	4.020997
249.706488	5553.367271	7.819507	-0.049532	4.023854
250.186175	5561.392769	7.824512	-0.049627	4.026727
250.337966	5569.417456	7.829517	-0.049660	4.029592
250.884436	5577.456946	7.834522	-0.049767	4.032467
251.342463	5585.488048	7.839526	-0.049858	4.035335
251.607270	5593.439109	7.844531	-0.049912	4.038169
252.086945	5601.437929	7.849536	-0.050007	4.041022
252.343553	5609.433358	7.854541	-0.050059	4.043868
252.276514	5617.516799	7.859546	-0.050052	4.046738
252.646181	5625.530964	7.864550	-0.050126	4.049589
253.038095	5633.543783	7.869555	-0.050204	4.052437
253.156011	5641.591318	7.874560	-0.050232	4.055291
253.128096	5649.634271	7.879565	-0.050232	4.058139
253.692818	5657.601199	7.884570	-0.050342	4.060968
254.390210	5665.575177	7.889574	-0.050477	4.063799
254.097654	5673.711302	7.894579	-0.050428	4.066670
254.519010	5681.680576	7.899584	-0.050511	4.069491
255.393637	5689.705881	7.904589	-0.050679	4.072337
255.396671	5697.776448	7.909594	-0.050685	4.075183
255.660604	5705.775030	7.914598	-0.050739	4.078006
255.816460	5713.753729	7.919603	-0.050774	4.080818
255.981922	5721.757119	7.924608	-0.050810	4.083637
256.034629	5729.834817	7.929613	-0.050825	4.086479
256.291247	5737.812730	7.934618	-0.050877	4.089287
256.365966	5745.933686	7.939622	-0.050897	4.092140
256.412752	5753.891546	7.944627	-0.050910	4.094933
256.453476	5761.942385	7.949632	-0.050923	4.097757
257.329566	5769.871650	7.954637	-0.051092	4.100549
257.399295	5777.876375	7.959642	-0.051110	4.103354
257.607870	5785.942507	7.964646	-0.051154	4.106180
258.064964	5793.918455	7.969651	-0.051244	4.108976
258.472702	5802.013731	7.974656	-0.051325	4.111811
258.557258	5810.018702	7.979661	-0.051346	4.114608
258.651559	5818.046667	7.984666	-0.051369	4.117411
259.254226	5826.025838	7.989670	-0.051486	4.120203
259.070698	5834.082220	7.994675	-0.051457	4.123008
259.357138	5842.027713	7.999680	-0.051516	4.125779
259.473208	5850.123552	8.004685	-0.051543	4.128599
259.813160	5858.154269	8.009690	-0.051611	4.131397
259.873144	5866.166436	8.014694	-0.051627	4.134183
259.785698	5874.219421	8.019699	-0.051616	4.136979
260.263172	5882.195772	8.024704	-0.051710	4.139754
260.595579	5890.219256	8.029709	-0.051777	4.142541
260.872262	5898.160322	8.034714	-0.051834	4.145298
261.039326	5906.245286	8.039718	-0.051870	4.148101
260.681454	5914.337574	8.044723	-0.051809	4.150897
261.150635	5922.243418	8.049728	-0.051901	4.153639
261.632581	5930.267128	8.054733	-0.051996	4.156419
261.672902	5938.253174	8.059738	-0.052009	4.159178
261.662729	5946.369437	8.064742	-0.052012	4.161980
261.545534	5954.336703	8.069747	-0.051996	4.164728
261.990519	5962.343868	8.074752	-0.052084	4.167494
262.494128	5970.353505	8.079757	-0.052183	4.170260
262.534299	5978.382733	8.084762	-0.052195	4.173025
262.853733	5986.467157	8.089766	-0.052260	4.175811
262.600757	5994.477715	8.094771	-0.052218	4.178562
263.145959	6002.460482	8.099776	-0.052325	4.181312
263.503018	6010.409019	8.104781	-0.052396	4.184046
263.428230	6018.535558	8.109786	-0.052388	4.186834
263.775713	6026.570740	8.114790	-0.052458	4.189594
264.029564	6034.612810	8.119795	-0.052510	4.192353
265.010284	6042.543928	8.124800	-0.052698	4.195081
264.558912	6050.643090	8.129805	-0.052619	4.197848
264.913596	6058.589243	8.134810	-0.052690	4.200570
264.887534	6066.619453	8.139814	-0.052691	4.203315
265.074074	6074.648623	8.144819	-0.052731	4.206059
265.291469	6082.612554	8.149824	-0.052776	4.208781
265.646613	6090.711697	8.154829	-0.052847	4.211548
266.185190	6098.626089	8.159834	-0.052953	4.214252
266.453653	6106.715143	8.164838	-0.053008	4.217011
266.607672	6114.672116	8.169843	-0.053042	4.219722
266.809060	6122.710746	8.174848	-0.053085	4.222459
267.039304	6130.753746	8.179853	-0.053133	4.225196
267.416765	6138.764222	8.184858	-0.053208	4.227923
267.742371	6146.844233	8.189862	-0.053274	4.230670
267.847662	6154.816112	8.194867	-0.053299	4.233376
267.964922	6162.863669	8.199872	-0.053326	4.236107
267.929752	6170.861384	8.204877	-0.053324	4.238817
268.415231	6178.856200	8.209882	-0.053420	4.241530
268.306561	6186.955106	8.214886	-0.053405	4.244270
268.375118	6194.942937	8.219891	-0.053423	4.246973
269.001646	6202.841138	8.224896	-0.053545	4.249649
269.185954	6210.931881	8.229901	-0.053584	4.252385
269.783473	6218.892347	8.234906	-0.053701	4.255078
269.521810	6227.079323	8.239910	-0.053657	4.257838
269.718476	6235.007698	8.244915	-0.053699	4.260513
269.696777	6243.048666	8.249920	-0.053700	4.263222
270.062338	6251.068458	8.254925	-0.053773	4.265927
270.311748	6259.024523	8.259930	-0.053825	4.268607
270.740084	6267.103051	8.264934	-0.053910	4.271328
270.561869	6275.131085	8.269939	-0.053882	4.274024
270.901689	6283.147352	8.274944	-0.053950	4.276720
270.947696	6291.155826	8.279949	-0.053964	4.279409
270.836213	6299.122632	8.284954	-0.053948	4.282080
271.195544	6307.118357	8.289958	-0.054021	4.284764
271.543944	6315.123284	8.294963	-0.054091	4.287449
272.053757	6323.127023	8.299968	-0.054191	4.290134
272.923305	6331.121391	8.304973	-0.054358	4.292817
272.838416	6339.184649	8.309978	-0.054347	4.295513
273.352838	6347.218874	8.314982	-0.054448	4.298202
273.870116	6355.170372	8.319987	-0.054550	4.300863
274.229697	6363.184576	8.324992	-0.054622	4.303541
274.432179	6371.337319	8.329997	-0.054665	4.306262
274.442756	6379.371092	8.335002	-0.054672	4.308940
274.605957	6387.406807	8.340006	-0.054707	4.311618
275.021789	6395.255278	8.345011	-0.054790	4.314235
274.849143	6403.376393	8.350016	-0.054763	4.316935
274.997201	6411.367508	8.355021	-0.054796	4.319594
275.300742	6419.382208	8.360026	-0.054857	4.322259
275.323643	6427.397794	8.365030	-0.054867	4.324922
275.708085	6435.404565	8.370035	-0.054944	4.327582
275.774307	6443.430934	8.375040	-0.054961	4.330245
276.154341	6451.477143	8.380045	-0.055037	4.332915
276.498483	6459.403973	8.385050	-0.055106	4.335544
276.939467	6467.439058	8.390054	-0.055194	4.338208
276.999628	6475.505435	8.395059	-0.055210	4.340877
277.295694	6483.470110	8.400064	-0.055270	4.343513
277.678257	6491.497239	8.405069	-0.055347	4.346168
278.115766	6499.507343	8.410074	-0.055433	4.348817
278.381100	6507.622100	8.415078	-0.055488	4.351497
278.266691	6515.631455	8.420083	-0.055472	4.354138
278.462104	6523.678322	8.425088	-0.055514	4.356792
278.457801	6531.629497	8.430093	-0.055518	4.359412
278.134762	6539.672321	8.435098	-0.055463	4.362057
278.135960	6547.638630	8.440102	-0.055468	4.364678
278.194228	6555.676849	8.445107	-0.055484	4.367322
278.739754	6563.641800	8.450112	-0.055591	4.369944
278.654549	6571.772870	8.455117	-0.055580	4.372614
278.656950	6579.702436	8.460122	-0.055586	4.375216
279.293144	6587.750753	8.465126	-0.055710	4.377861
279.220022	6595.783025	8.470131	-0.055701	4.380494
279.123601	6603.825362	8.475136	-0.055688	4.383128
279.568473	6611.820243	8.480141	-0.055777	4.385749
279.585972	6619.777361	8.485146	-0.055785	4.388353
280.106785	6627.841628	8.490150	-0.055887	4.390994
280.537801	6635.760863	8.495155	-0.055972	4.393585
280.876555	6643.812040	8.500160	-0.056041	4.396218
281.377575	6651.790355	8.505165	-0.056139	4.398825
281.635900	6659.811875	8.510170	-0.056192	4.401444
281.538193	6667.854776	8.515174	-0.056179	4.404066
281.920706	6675.911414	8.520179	-0.056256	4.406694
282.220448	6683.903638	8.525184	-0.056317	4.409298
282.636686	6691.958010	8.530189	-0.056400	4.411922
282.425523	6699.998322	8.535194	-0.056365	4.414537
282.530796	6708.095127	8.540198	-0.056390	4.417169
283.076573	6715.995568	8.545203	-0.056497	4.419739
283.143487	6724.041242	8.550208	-0.056515	4.422352
283.165337	6732.117535	8.555213	-0.056524	4.424973
283.425930	6740.104863	8.560218	-0.056578	4.427565
283.937160	6748.130182	8.565223	-0.056678	4.430169
283.766555	6756.184744	8.570227	-0.056651	4.432777
284.059315	6764.233183	8.575232	-0.056711	4.435384
284.313482	6772.222463	8.580237	-0.056764	4.437971
284.455821	6780.223208	8.585242	-0.056795	4.440558
284.283131	6788.252240	8.590247	-0.056768	4.443152
284.193474	6796.285517	8.595251	-0.056757	4.445746
284.483988	6804.249610	8.600256	-0.056816	4.448318
285.138325	6812.323976	8.605261	-0.056943	4.450927
285.077982	6820.320619	8.610266	-0.056937	4.453504
285.076398	6828.408194	8.615271	-0.056942	4.456110
285.512405	6836.330885	8.620275	-0.057028	4.458664
285.582505	6844.356985	8.625280	-0.057047	4.461247
285.778525	6852.349969	8.630285	-0.057088	4.463819
285.554230	6860.451961	8.635290	-0.057052	4.466423
285.310374	6868.514170	8.640295	-0.057012	4.469012
286.036920	6876.422124	8.645299	-0.057152	4.471554
286.580194	6884.393911	8.650304	-0.057258	4.474115
286.937782	6892.468506	8.655309	-0.057330	4.476706
286.820988	6900.425851	8.660314	-0.057313	4.479256
287.029883	6908.535350	8.665319	-0.057358	4.481855
287.049682	6916.494157	8.670323	-0.057366	4.484403
287.000241	6924.579440	8.675328	-0.057362	4.486990
287.018753	6932.576700	8.680333	-0.057371	4.489548
287.434412	6940.579317	8.685338	-0.057454	4.492107
287.816426	6948.531368	8.690343	-0.057530	4.494649
287.591342	6956.612016	8.695347	-0.057493	4.497227
288.073392	6964.598541	8.700352	-0.057588	4.499777
288.359094	6972.649935	8.705357	-0.057646	4.502346
288.126860	6980.632794	8.710362	-0.057608	4.504889
288.472391	6988.716314	8.715367	-0.057678	4.507465
288.493458	6996.739639	8.720371	-0.057687	4.510019
289.047478	7004.642769	8.725376	-0.057795	4.512536
289.118330	7012.693369	8.730381	-0.057814	4.515096
289.146240	7020.707766	8.735386	-0.057824	4.517643
289.652449	7028.693097	8.740391	-0.057924	4.520180
290.027763	7036.680556	8.745395	-0.057999	4.522717
290.536285	7044.633882	8.750400	-0.058098	4.525242
290.596354	7052.763813	8.755405	-0.058115	4.527820
290.440118	7060.762568	8.760410	-0.058091	4.530354
290.971680	7068.794597	8.765415	-0.058195	4.532899
291.108005	7076.799583	8.770419	-0.058226	4.535433
291.322882	7084.786660	8.775424	-0.058271	4.537961
291.608706	7092.840854	8.780429	-0.058329	4.540508
291.505302	7100.849782	8.785434	-0.058315	4.543038
292.077710	7108.866167	8.790439	-0.058427	4.545571
291.919764	7116.904347	8.795443	-0.058403	4.548108
292.542987	7124.871176	8.800448	-0.058524	4.550623
292.435294	7132.952597	8.805453	-0.058509	4.553170
292.843411	7140.894684	8.810458	-0.058590	4.555674
293.427104	7148.890526	8.815463	-0.058704	4.558193
293.613067	7156.972406	8.820467	-0.058744	4.560737
293.178713	7164.984995	8.825472	-0.058668	4.563257
293.507960	7172.930846	8.830477	-0.058735	4.565756
293.598397	7180.962351	8.835482	-0.058757	4.568280
294.318519	7189.028901	8.840487	-0.058896	4.570814
294.139919	7197.062324	8.845491	-0.058868	4.573335
293.848828	7205.146626	8.850496	-0.058819	4.575871
294.163414	7213.156871	8.855501	-0.058883	4.578383
294.559146	7221.104388	8.860506	-0.058961	4.580874
295.072090	7229.021813	8.865511	-0.059062	4.583354
295.300509	7237.121919	8.870515	-0.059110	4.585890
295.015101	7245.184445	8.875520	-0.059062	4.588411
295.147532	7253.254131	8.880525	-0.059092	4.590935
295.450662	7261.161567	8.885530	-0.059153	4.593406
295.852976	7269.241901	8.890535	-0.059234	4.595930
296.005046	7277.201932	8.895539	-0.059267	4.598415
296.372875	7285.232454	8.900544	-0.059341	4.600921
296.657076	7293.203757	8.905549	-0.059399	4.603406
296.959992	7301.157363	8.910554	-0.059460	4.605885
297.516910	7309.175576	8.915559	-0.059569	4.608383
297.952665	7317.237932	8.920563	-0.059655	4.610893
297.537096	7325.339893	8.925568	-0.059583	4.613413
297.955163	7333.320910	8.930573	-0.059666	4.615895
298.017067	7341.308477	8.935578	-0.059683	4.618378
298.788886	7349.305399	8.940583	-0.059832	4.620862
298.446627	7357.300821	8.945587	-0.059773	4.623344
298.619778	7365.375650	8.950592	-0.059811	4.625849
298.799890	7373.407583	8.955597	-0.059850	4.628340
298.632249	7381.453704	8.960602	-0.059824	4.630834
299.104815	7389.425284	8.965607	-0.059917	4.633303
299.387795	7397.446008	8.970611	-0.059975	4.635786
299.683024	7405.417641	8.975616	-0.060035	4.638253
299.804857	7413.483735	8.980621	-0.060063	4.640747
299.765954	7421.409918	8.985626	-0.060060	4.643197
300.123430	7429.501670	8.990631	-0.060132	4.645697
300.124591	7437.485903	8.995635	-0.060138	4.648162
300.308127	7445.527928	9.000640	-0.060177	4.650644
300.640351	7453.513532	9.005645	-0.060244	4.653107
300.660415	7461.538994	9.010650	-0.060253	4.655581
300.863281	7469.581933	9.015655	-0.060296	4.658059
301.219683	7477.583649	9.020659	-0.060367	4.660523
301.927621	7485.531060	9.025664	-0.060504	4.662968
302.117738	7493.638928	9.030669	-0.060545	4.665462
302.407702	7501.625343	9.035674	-0.060604	4.667917
302.549671	7509.649464	9.040679	-0.060636	4.670383
302.719920	7517.685042	9.045683	-0.060673	4.672850
303.157140	7525.687686	9.050688	-0.060759	4.675306
303.206053	7533.726649	9.055693	-0.060774	4.677773
303.436294	7541.702995	9.060698	-0.060822	4.680218
303.248489	7549.776507	9.065703	-0.060792	4.682692
303.111305	7557.713635	9.070707	-0.060771	4.685123
303.688674	7565.742266	9.075712	-0.060884	4.687581
303.984691	7573.735819	9.080717	-0.060944	4.690026
304.000239	7581.801295	9.085722	-0.060953	4.692492
303.923404	7589.839075	9.090727	-0.060943	4.694949
304.356354	7597.819300	9.095731	-0.061029	4.697387
304.464764	7605.783305	9.100736	-0.061055	4.699818
305.017415	7613.838023	9.105741	-0.061163	4.702275
304.926638	7621.809749	9.110746	-0.061151	4.704707
305.459994	7629.883337	9.115751	-0.061255	4.707167
305.443931	7637.938562	9.120755	-0.061258	4.709621
305.353529	7645.975104	9.125760	-0.061246	4.712069
305.749888	7653.908238	9.130765	-0.061325	4.714483
305.959886	7661.949420	9.135770	-0.061369	4.716928
306.145519	7669.931062	9.140775	-0.061409	4.719355
306.102964	7678.040059	9.145779	-0.061406	4.721819
306.555748	7685.974976	9.150784	-0.061496	4.724228
306.763905	7694.108226	9.155789	-0.061540	4.726697
307.790122	7701.952033	9.160794	-0.061736	4.729075
307.659150	7710.105341	9.165799	-0.061717	4.731547
308.159791	7718.042134	9.170803	-0.061815	4.733952
308.257041	7726.073385	9.175808	-0.061838	4.736385
308.274624	7734.141296	9.180813	-0.061847	4.738827
308.388134	7742.167591	9.185818	-0.061873	4.741256
308.868137	7750.125220	9.190823	-0.061968	4.743662
309.462134	7758.096157	9.195827	-0.062083	4.746070
309.603260	7766.159019	9.200832	-0.062115	4.748506
309.569044	7774.303359	9.205837	-0.062114	4.750965
310.485274	7782.178855	9.210842	-0.062290	4.753340
310.407086	7790.288876	9.215847	-0.062280	4.755787
310.455604	7798.268400	9.220851	-0.062294	4.758193
311.017045	7806.222049	9.225856	-0.062404	4.760588
311.204848	7814.294946	9.230861	-0.062444	4.763019
311.314458	7822.230295	9.235866	-0.062470	4.765408
311.462070	7830.273796	9.240871	-0.062502	4.767828
311.938802	7838.320283	9.245875	-0.062596	4.770247
312.069255	7846.333550	9.250880	-0.062626	4.772655
312.408428	7854.317558	9.255885	-0.062694	4.775053
312.296165	7862.394950	9.260890	-0.062679	4.777478
313.032482	7870.325585	9.265895	-0.062821	4.779856
313.238004	7878.350896	9.270899	-0.062864	4.782263
313.419805	7886.364470	9.275904	-0.062903	4.784665
313.423378	7894.498042	9.280909	-0.062909	4.787103
313.363846	7902.472450	9.285914	-0.062903	4.789491
313.735962	7910.505571	9.290919	-0.062978	4.791895
313.770707	7918.475491	9.295923	-0.062989	4.794279
314.138940	7926.517884	9.300928	-0.063063	4.796683
314.390331	7934.506711	9.305933	-0.063115	4.799070
314.754977	7942.533339	9.310938	-0.063188	4.801467
315.105994	7950.434286	9.315943	-0.063259	4.803825
315.590434	7958.516640	9.320947	-0.063354	4.806236
315.280498	7966.588315	9.325952	-0.063302	4.808645
315.098442	7974.695887	9.330957	-0.063273	4.811063
314.957271	7982.612036	9.335962	-0.063252	4.813422
315.204181	7990.047390	9.340967	-0.063303	4.815636
315.587433	7994.681525	9.345971	-0.063377	4.817015

315.873436	7997.212734	9.350976	-0.063432	4.817767
315.843608	7998.466814	9.355981	-0.063427	4.818140
316.128693	7998.857574	9.360986	-0.063480	4.818256
316.779859	7999.843709	9.365991	-0.063602	4.818546
316.599551	7999.891712	9.370995	-0.063568	4.818561
316.879736	7999.826121	9.376000	-0.063621	4.818541
317.448327	7999.793658	9.381005	-0.063726	4.818529
316.853158	7999.844651	9.386010	-0.063616	4.818546
317.810913	7999.778442	9.391015	-0.063794	4.818523
318.119441	7999.691190	9.396019	-0.063851	4.818496
318.078262	7999.727367	9.401024	-0.063843	4.818507
317.688281	7999.792572	9.406029	-0.063771	4.818528
317.663055	7999.761817	9.411034	-0.063766	4.818519
318.167131	7999.800902	9.416039	-0.063860	4.818528
317.749065	7999.731460	9.421043	-0.063782	4.818509
318.155250	7999.714717	9.426048	-0.063858	4.818503
318.222819	7999.765949	9.431053	-0.063870	4.818518
318.167161	7999.762074	9.436058	-0.063860	4.818517
318.230451	7999.785975	9.441063	-0.063871	4.818524
318.181317	7999.789528	9.446067	-0.063862	4.818525
318.497760	7999.806237	9.451072	-0.063921	4.818529
318.465281	7999.826793	9.456077	-0.063915	4.818535
318.527797	7999.757316	9.461082	-0.063927	4.818514
318.519029	7999.814898	9.466087	-0.063925	4.818531
317.903860	7999.921228	9.471091	-0.063810	4.818565
318.340362	7999.835643	9.476096	-0.063892	4.818538
319.057547	7999.804073	9.481101	-0.064025	4.818526
318.664883	7999.819934	9.486106	-0.063952	4.818532
318.568798	7999.847004	9.491111	-0.063934	4.818541
318.498190	7999.870209	9.496115	-0.063921	4.818548
318.697513	7999.823497	9.501120	-0.063958	4.818533
318.617048	7999.893783	9.506125	-0.063943	4.818554
318.687213	7999.817062	9.511130	-0.063956	4.818531
318.685113	7999.863191	9.516135	-0.063956	4.818545
318.958948	7999.808008	9.521139	-0.064006	4.818527
318.999315	7999.831611	9.526144	-0.064014	4.818534
319.031583	7999.893926	9.531149	-0.064020	4.818553
319.427935	7999.804671	9.536154	-0.064094	4.818525
319.714415	7999.789519	9.541159	-0.064147	4.818519
320.086912	7999.741917	9.546163	-0.064216	4.818503
319.818958	7999.763599	9.551168	-0.064166	4.818511
319.624581	7999.841843	9.556173	-0.064130	4.818535
319.185880	7999.792058	9.561178	-0.064048	4.818522
319.692798	7999.790271	9.566183	-0.064143	4.818519
319.721346	7999.754970	9.571187	-0.064148	4.818509
319.757077	7999.778514	9.576192	-0.064155	4.818516
320.023607	7999.789330	9.581197	-0.064204	4.818518
319.740448	7999.768849	9.586202	-0.064151	4.818513
319.906120	7999.785693	9.591207	-0.064182	4.818517
320.143846	7999.762562	9.596211	-0.064226	4.818509
320.323566	7999.777493	9.601216	-0.064260	4.818513
320.055620	7999.797076	9.606221	-0.064210	4.818520
320.278939	7999.743333	9.611226	-0.064251	4.818503
319.958791	7999.841968	9.616231	-0.064192	4.818534
319.957250	7999.803127	9.621235	-0.064191	4.818522
319.861939	7999.780899	9.626240	-0.064174	4.818516
320.222234	7999.754121	9.631245	-0.064241	4.818507
320.288258	7999.752881	9.636250	-0.064253	4.818506
320.417048	7999.782884	9.641255	-0.064277	4.818514
320.425019	7999.766199	9.646259	-0.064278	4.818509
320.639453	7999.765845	9.651264	-0.064318	4.818508
320.707899	7999.768833	9.656269	-0.064331	4.818509
320.521550	7999.753810	9.661274	-0.064296	4.818505
320.239111	7999.797334	9.666279	-0.064244	4.818519
320.131501	7999.756061	9.671283	-0.064223	4.818507
319.827603	7999.807698	9.676288	-0.064167	4.818524
320.312912	7999.759469	9.681293	-0.064257	4.818508
320.394687	7999.741649	9.686298	-0.064272	4.818502
319.914912	7999.832957	9.691303	-0.064183	4.818531
319.933730	7999.800676	9.696307	-0.064186	4.818522
320.186183	7999.784032	9.701312	-0.064233	4.818516
320.468578	7999.798204	9.706317	-0.064286	4.818519
320.329258	7999.744977	9.711322	-0.064260	4.818503
320.842489	7999.743275	9.716327	-0.064355	4.818501
320.801867	7999.889621	9.721331	-0.064348	4.818545
320.681094	7999.776834	9.726336	-0.064325	4.818512
320.841072	7999.766328	9.731341	-0.064355	4.818508
320.679119	7999.847094	9.736346	-0.064325	4.818532
320.803001	7999.842412	9.741351	-0.064348	4.818531
320.295760	7999.779139	9.746355	-0.064253	4.818514
320.384653	7999.808622	9.751360	-0.064270	4.818522
320.139081	8000.037273	9.756365	-0.064224	4.818591
320.100106	7999.840575	9.761370	-0.064217	4.818533
320.486230	7999.814134	9.766375	-0.064289	4.818523
321.029885	7999.825420	9.771379	-0.064390	4.818525
320.464811	7999.855814	9.776384	-0.064285	4.818536
320.715510	7999.748922	9.781389	-0.064331	4.818503
320.759347	7999.829225	9.786394	-0.064339	4.818527
320.650983	7999.868725	9.791399	-0.064319	4.818539
321.169386	7999.744343	9.796403	-0.064416	4.818500
321.270461	7999.953391	9.801408	-0.064434	4.818562
321.003282	7999.813511	9.806413	-0.064385	4.818521
320.908803	7999.860536	9.811418	-0.064367	4.818536
321.104849	7999.769717	9.816423	-0.064403	4.818508
321.299082	7999.837296	9.821427	-0.064440	4.818527
320.764914	7999.817733	9.826432	-0.064340	4.818523
321.161974	7999.788289	9.831437	-0.064414	4.818513
320.940746	7999.835758	9.836442	-0.064373	4.818528
321.304828	7999.804835	9.841447	-0.064440	4.818517
321.350550	7999.870476	9.846451	-0.064449	4.818537
321.302975	7999.855164	9.851456	-0.064440	4.818532
321.125460	7999.808780	9.856461	-0.064407	4.818519
321.063733	7999.764957	9.861466	-0.064395	4.818507
320.734164	7999.800521	9.866471	-0.064334	4.818518
321.038268	7999.757274	9.871475	-0.064390	4.818504
320.953246	7999.849535	9.876480	-0.064375	4.818532
320.911061	7999.798623	9.881485	-0.064367	4.818517
320.880218	7999.778284	9.886490	-0.064361	4.818511
320.907116	7999.788074	9.891495	-0.064366	4.818514
320.409099	7999.866554	9.896499	-0.064273	4.818539
320.553685	7999.822275	9.901504	-0.064300	4.818526
320.917823	7999.790303	9.906509	-0.064368	4.818515
320.403586	7999.809820	9.911514	-0.064272	4.818522
320.746084	7999.822678	9.916519	-0.064336	4.818525
320.708460	7999.920803	9.921523	-0.064329	4.818554
320.640843	7999.830741	9.926528	-0.064316	4.818528
320.518382	7999.878449	9.931533	-0.064293	4.818542
321.353915	7999.971184	9.936538	-0.064449	4.818567
321.245386	7999.833374	9.941543	-0.064428	4.818526
320.958034	7999.895717	9.946547	-0.064375	4.818546
320.931183	7999.797793	9.951552	-0.064370	4.818517
321.241782	7999.830170	9.956557	-0.064428	4.818525
321.218246	7999.780550	9.961562	-0.064423	4.818511
321.289899	7999.787777	9.966567	-0.064437	4.818512
321.033046	7999.826388	9.971571	-0.064389	4.818525
321.102214	7999.772732	9.976576	-0.064401	4.818509
321.302686	7999.891800	9.981581	-0.064439	4.818543
321.055968	7999.766877	9.986586	-0.064393	4.818507
321.224865	7999.775372	9.991591	-0.064424	4.818509
321.247439	7999.777762	9.996595	-0.064428	4.818510
320.756407	7999.926625	10.001600	-0.064337	4.818556
321.449991	7999.774104	10.006605	-0.064466	4.818508
320.801671	7999.808656	10.011610	-0.064345	4.818521
321.714341	7999.756565	10.016615	-0.064515	4.818502
321.743609	7999.837729	10.021619	-0.064521	4.818526
321.865674	7999.753288	10.026624	-0.064543	4.818500
321.802573	7999.765051	10.031629	-0.064531	4.818504
321.626640	7999.858225	10.036634	-0.064499	4.818532
321.729259	7999.775629	10.041639	-0.064518	4.818507
321.738243	7999.746367	10.046643	-0.064519	4.818498
322.059433	7999.843932	10.051648	-0.064579	4.818526
321.913009	7999.776969	10.056653	-0.064552	4.818507
321.887184	7999.850070	10.061658	-0.064547	4.818529
321.721137	7999.760819	10.066663	-0.064516	4.818503
321.907936	7999.856630	10.071667	-0.064551	4.818531
321.318717	7999.787036	10.076672	-0.064441	4.818512
321.343603	7999.780014	10.081677	-0.064446	4.818510
321.481417	7999.859446	10.086682	-0.064471	4.818533
322.063863	7999.835572	10.091687	-0.064580	4.818524
321.938716	7999.842328	10.096691	-0.064556	4.818526
321.612618	7999.791905	10.101696	-0.064495	4.818512
321.909873	7999.796831	10.106701	-0.064551	4.818513
321.908919	7999.852422	10.111706	-0.064551	4.818529
322.124538	7999.768153	10.116711	-0.064591	4.818503
322.332885	7999.845361	10.121715	-0.064629	4.818526
322.596599	7999.829916	10.126720	-0.064678	4.818520
322.490234	7999.829573	10.131725	-0.064659	4.818520
322.244045	7999.830552	10.136730	-0.064613	4.818522
322.330437	7999.855808	10.141735	-0.064629	4.818529
322.034010	7999.756461	10.146739	-0.064573	4.818500
321.795434	7999.768032	10.151744	-0.064529	4.818505
322.148859	7999.884903	10.156749	-0.064595	4.818538
321.480476	7999.805881	10.161754	-0.064470	4.818517
321.064788	7999.872845	10.166759	-0.064393	4.818539
321.567785	7999.838489	10.171763	-0.064487	4.818526
321.346733	7999.820913	10.176768	-0.064445	4.818522
322.061047	7999.793513	10.181773	-0.064578	4.818511
322.034449	7999.847719	10.186778	-0.064573	4.818527
322.034467	7999.775324	10.191783	-0.064573	4.818506
322.057484	7999.853260	10.196787	-0.064577	4.818529
322.411228	7999.856826	10.201792	-0.064643	4.818529
322.742410	7999.831771	10.206797	-0.064705	4.818520
322.275016	7999.836156	10.211802	-0.064618	4.818523
322.409139	7999.749774	10.216807	-0.064643	4.818497
322.254399	7999.776078	10.221811	-0.064614	4.818505
322.378068	7999.899394	10.226816	-0.064637	4.818541
322.010355	7999.792820	10.231821	-0.064568	4.818511
322.018555	7999.747810	10.236826	-0.064570	4.818498
321.979284	7999.889981	10.241831	-0.064563	4.818540
322.406518	7999.839950	10.246835	-0.064642	4.818524
322.581539	7999.925118	10.251840	-0.064675	4.818548
322.502424	7999.826508	10.256845	-0.064660	4.818519
322.600783	7999.830937	10.261850	-0.064678	4.818520
322.619350	7999.735701	10.266855	-0.064681	4.818492
322.563817	7999.860874	10.271859	-0.064671	4.818529
322.383364	7999.755696	10.276864	-0.064637	4.818499
322.416139	7999.852645	10.281869	-0.064644	4.818527
322.722894	7999.815729	10.286874	-0.064701	4.818515
322.892330	7999.946990	10.291879	-0.064732	4.818554
322.976214	7999.730900	10.296883	-0.064748	4.818489
322.648169	7999.832580	10.301888	-0.064687	4.818521
322.587431	7999.858014	10.306893	-0.064675	4.818528
322.575672	7999.744546	10.311898	-0.064673	4.818495
322.644257	7999.760127	10.316903	-0.064686	4.818499
322.489172	7999.854623	10.321907	-0.064657	4.818528
322.342174	7999.764570	10.326912	-0.064629	4.818502
322.418329	7999.758217	10.331917	-0.064643	4.818499
322.271355	7999.863310	10.336922	-0.064616	4.818531
322.271968	7999.800365	10.341927	-0.064616	4.818512
322.617235	7999.748214	10.346931	-0.064680	4.818496
322.451514	7999.835227	10.351936	-0.064649	4.818522
322.431799	7999.786705	10.356941	-0.064646	4.818508
322.481411	7999.759022	10.361946	-0.064655	4.818499
322.822950	7999.873643	10.366951	-0.064719	4.818532
322.452442	7999.727162	10.371955	-0.064649	4.818490
322.356132	7999.870688	10.376960	-0.064632	4.818533
322.485631	7999.750671	10.381965	-0.064656	4.818497
322.466828	7999.845898	10.386970	-0.064652	4.818525
322.311802	7999.871149	10.391975	-0.064623	4.818533
322.749182	7999.759349	10.396979	-0.064704	4.818498
322.764802	7999.855026	10.401984	-0.064707	4.818527
322.632617	7999.784050	10.406989	-0.064683	4.818506
322.340840	7999.763451	10.411994	-0.064628	4.818501
322.513339	7999.798224	10.416999	-0.064660	4.818511
322.496397	7999.863049	10.422003	-0.064657	4.818530
322.574274	7999.761243	10.427008	-0.064672	4.818500
322.612500	7999.820494	10.432013	-0.064679	4.818517
322.439683	7999.853906	10.437018	-0.064647	4.818528
322.792367	7999.853263	10.442023	-0.064712	4.818526
322.487624	7999.749608	10.447027	-0.064655	4.818497
322.544973	7999.861567	10.452032	-0.064666	4.818530
322.291171	7999.792151	10.457037	-0.064619	4.818510
322.356341	7999.885327	10.462042	-0.064631	4.818537
322.357907	7999.804557	10.467047	-0.064631	4.818513
322.263931	7999.812770	10.472051	-0.064613	4.818516
322.332294	7999.757004	10.477056	-0.064626	4.818499
322.741655	7999.775985	10.482061	-0.064702	4.818503
322.841916	7999.843390	10.487066	-0.064721	4.818523
322.453674	7999.778514	10.492071	-0.064649	4.818505
322.269846	7999.851651	10.497075	-0.064614	4.818528
321.580310	7999.880416	10.502080	-0.064486	4.818539
322.097472	7999.841001	10.507085	-0.064582	4.818525
322.015108	7999.794808	10.512090	-0.064567	4.818512
322.349211	7999.796020	10.517095	-0.064629	4.818511
322.474648	7999.811294	10.522099	-0.064652	4.818515
322.011004	7999.874482	10.527104	-0.064566	4.818536
322.076444	7999.867990	10.532109	-0.064578	4.818533
322.149340	7999.872086	10.537114	-0.064592	4.818534
322.141820	7999.864640	10.542119	-0.064590	4.818532
322.156284	7999.856433	10.547123	-0.064593	4.818530
322.235824	7999.825993	10.552128	-0.064608	4.818520
322.112175	7999.846408	10.557133	-0.064585	4.818527
322.354941	7999.812854	10.562138	-0.064630	4.818516
322.177329	7999.816827	10.567143	-0.064597	4.818518
321.922208	7999.959327	10.572147	-0.064549	4.818561
321.758304	7999.856464	10.577152	-0.064518	4.818531
322.326059	7999.793579	10.582157	-0.064624	4.818510
322.033887	7999.803401	10.587162	-0.064570	4.818514
321.906409	7999.824815	10.592167	-0.064546	4.818521
322.062879	7999.850986	10.597171	-0.064575	4.818528
322.226990	7999.819552	10.602176	-0.064605	4.818518
322.152792	7999.865793	10.607181	-0.064592	4.818532
322.144834	7999.856243	10.612186	-0.064590	4.818530
322.696326	7999.814130	10.617191	-0.064693	4.818515
322.676513	7999.808622	10.622195	-0.064689	4.818513
322.424655	7999.782249	10.627200	-0.064642	4.818507
322.531508	7999.807772	10.632205	-0.064662	4.818514
321.967178	7999.827679	10.637210	-0.064557	4.818522
322.304150	7999.802699	10.642215	-0.064619	4.818513
322.493838	7999.896451	10.647219	-0.064655	4.818540
322.673690	7999.746665	10.652224	-0.064688	4.818495
322.553916	7999.790213	10.657229	-0.064666	4.818508
322.778031	7999.838252	10.662234	-0.064708	4.818522
322.594334	7999.791784	10.667239	-0.064673	4.818509
322.531183	7999.832923	10.672243	-0.064662	4.818521
322.857640	7999.780528	10.677248	-0.064722	4.818504
322.584069	7999.857739	10.682253	-0.064671	4.818528
322.617904	7999.808866	10.687258	-0.064678	4.818514
322.728444	7999.791421	10.692263	-0.064698	4.818508
322.321170	7999.864788	10.697267	-0.064622	4.818531
321.990210	7999.870956	10.702272	-0.064561	4.818535
322.213814	7999.878069	10.707277	-0.064602	4.818536
322.563492	7999.913059	10.712282	-0.064667	4.818545
322.784674	7999.803681	10.717287	-0.064708	4.818512
322.738900	7999.805179	10.722291	-0.064700	4.818512
322.563026	7999.783994	10.727296	-0.064667	4.818507
322.728511	7999.809234	10.732301	-0.064698	4.818513
322.612580	7999.787782	10.737306	-0.064676	4.818507
322.749851	7999.812654	10.742311	-0.064702	4.818514
322.763329	7999.786597	10.747315	-0.064704	4.818507
322.782983	7999.762720	10.752320	-0.064708	4.818499
322.516177	7999.890380	10.757325	-0.064658	4.818538
322.445047	7999.808661	10.762330	-0.064645	4.818514
322.483806	7999.842738	10.767335	-0.064652	4.818524
322.420367	7999.846103	10.772339	-0.064640	4.818526
322.133169	7999.804580	10.777344	-0.064586	4.818514
322.330244	7999.831281	10.782349	-0.064623	4.818522
322.304371	7999.805760	10.787354	-0.064618	4.818514
322.260969	7999.795748	10.792359	-0.064610	4.818511
322.145143	7999.886559	10.797363	-0.064589	4.818539
322.375590	7999.809828	10.802368	-0.064631	4.818515
322.642535	7999.874163	10.807373	-0.064681	4.818533
322.125551	7999.832787	10.812378	-0.064585	4.818523
322.372315	7999.876923	10.817383	-0.064631	4.818535
322.468804	7999.832016	10.822387	-0.064649	4.818521
322.247864	7999.827030	10.827392	-0.064607	4.818521
322.595954	7999.844162	10.832397	-0.064672	4.818524
322.462485	7999.863400	10.837402	-0.064647	4.818531
322.491069	7999.802918	10.842407	-0.064653	4.818512
322.559611	7999.793318	10.847411	-0.064665	4.818509
322.124790	7999.825408	10.852416	-0.064584	4.818521
322.373788	7999.867475	10.857421	-0.064631	4.818532
322.424594	7999.835611	10.862426	-0.064640	4.818522
322.466751	7999.871831	10.867431	-0.064648	4.818533
322.089669	7999.926707	10.872435	-0.064578	4.818551
322.043283	7999.886229	10.877440	-0.064569	4.818539
322.641445	7999.833185	10.882445	-0.064680	4.818521
322.353051	7999.864039	10.887450	-0.064626	4.818531
322.569883	7999.957097	10.892455	-0.064667	4.818558
322.068890	7999.920125	10.897459	-0.064574	4.818549
322.243194	7999.851054	10.902464	-0.064606	4.818528
322.590079	7999.830400	10.907469	-0.064670	4.818520
322.504994	7999.813548	10.912474	-0.064655	4.818516
322.577640	7999.843871	10.917479	-0.064668	4.818524
322.769724	7999.896738	10.922483	-0.064704	4.818539
322.226807	7999.884398	10.927488	-0.064603	4.818538
322.440482	7999.891382	10.932493	-0.064642	4.818539
322.926697	7999.786515	10.937498	-0.064733	4.818506
323.180569	7999.776189	10.942503	-0.064780	4.818502
323.260471	7999.896838	10.947507	-0.064795	4.818537
323.188558	7999.768942	10.952512	-0.064781	4.818500
323.594000	7999.777383	10.957517	-0.064857	4.818501
323.195070	7999.772169	10.962522	-0.064783	4.818501
322.999884	7999.894470	10.967527	-0.064746	4.818538
322.598988	7999.934346	10.972531	-0.064672	4.818551
322.460796	7999.843357	10.977536	-0.064646	4.818525
322.666463	7999.870171	10.982541	-0.064684	4.818532
322.928400	7999.808540	10.987546	-0.064733	4.818512
322.985108	7999.849147	10.992551	-0.064743	4.818524
322.852600	7999.848462	10.997555	-0.064719	4.818525
322.962489	7999.792189	11.002560	-0.064739	4.818507
323.290491	7999.777584	11.007565	-0.064800	4.818502
322.944539	7999.897916	11.012570	-0.064736	4.818539
322.829310	7999.848145	11.017575	-0.064714	4.818525
323.074922	7999.832465	11.022579	-0.064760	4.818519
323.247012	7999.804283	11.027584	-0.064792	4.818510
323.660426	7999.825419	11.032589	-0.064869	4.818515
323.459100	7999.800752	11.037594	-0.064831	4.818508
322.856016	7999.852676	11.042599	-0.064719	4.818526
322.849134	7999.857829	11.047603	-0.064717	4.818527
322.584718	7999.849126	11.052608	-0.064668	4.818526
323.156682	7999.826167	11.057613	-0.064775	4.818517
322.400235	7999.974711	11.062618	-0.064634	4.818564
322.797705	7999.872882	11.067623	-0.064708	4.818532
322.771966	7999.898773	11.072627	-0.064703	4.818540
322.863327	7999.837012	11.077632	-0.064720	4.818521
322.813262	7999.874126	11.082637	-0.064710	4.818532
322.966688	7999.879274	11.087642	-0.064739	4.818533
323.330355	7999.861989	11.092647	-0.064807	4.818527
323.264511	7999.871617	11.097651	-0.064794	4.818530
323.246875	7999.910204	11.102656	-0.064791	4.818541
323.655540	7999.821112	11.107661	-0.064867	4.818513
323.085800	7999.852486	11.112666	-0.064761	4.818525
322.437393	7999.934244	11.117671	-0.064640	4.818552
323.223641	7999.901495	11.122675	-0.064787	4.818539
323.176941	7999.823241	11.127680	-0.064778	4.818516
323.109645	7999.881114	11.132685	-0.064765	4.818533
323.426487	7999.813904	11.137690	-0.064824	4.818512
323.025796	7999.840143	11.142695	-0.064749	4.818522
323.435936	7999.808776	11.147699	-0.064826	4.818511
323.376401	7999.812192	11.152704	-0.064815	4.818512
323.406277	7999.816776	11.157709	-0.064820	4.818513
323.250569	7999.812640	11.162714	-0.064791	4.818512
323.276028	7999.814019	11.167719	-0.064796	4.818513
323.467731	7999.871079	11.172723	-0.064832	4.818529
323.305415	7999.831184	11.177728	-0.064801	4.818518
322.867719	7999.861136	11.182733	-0.064720	4.818528
323.174777	7999.834717	11.187738	-0.064777	4.818519
323.296742	7999.809028	11.192743	-0.064799	4.818511
323.427003	7999.838006	11.197747	-0.064824	4.818519
323.326326	7999.807310	11.202752	-0.064805	4.818511
323.670433	7999.824393	11.207757	-0.064869	4.818514
323.665076	7999.805434	11.212762	-0.064868	4.818509
323.691254	7999.803675	11.217767	-0.064873	4.818508
323.905109	7999.864173	11.222771	-0.064913	4.818525
323.518630	7999.797216	11.227776	-0.064840	4.818507
323.398187	7999.859641	11.232781	-0.064818	4.818526
323.196389	7999.842313	11.237786	-0.064780	4.818522
323.570120	7999.824110	11.242791	-0.064850	4.818515
323.238486	7999.873283	11.247795	-0.064788	4.818531
323.092341	7999.831502	11.252800	-0.064761	4.818519
323.409884	7999.833548	11.257805	-0.064820	4.818518
323.419346	7999.809537	11.262810	-0.064822	4.818511
323.429838	7999.828557	11.267815	-0.064824	4.818517
323.656706	7999.793747	11.272819	-0.064866	4.818505
323.621768	7999.813222	11.277824	-0.064859	4.818511
323.835237	7999.819156	11.282829	-0.064899	4.818512
323.549879	7999.820670	11.287834	-0.064846	4.818514
323.432270	7999.896772	11.292839	-0.064824	4.818537
323.655045	7999.818890	11.297843	-0.064865	4.818513
323.380314	7999.845725	11.302848	-0.064814	4.818522
323.878956	7999.828105	11.307853	-0.064907	4.818515
323.763603	7999.776233	11.312858	-0.064885	4.818500
323.924862	7999.796173	11.317863	-0.064915	4.818505
323.969600	7999.806198	11.322867	-0.064924	4.818508
323.557848	7999.901538	11.327872	-0.064847	4.818538
323.623629	7999.790130	11.332877	-0.064859	4.818504
323.669479	7999.766594	11.337882	-0.064868	4.818497
323.412919	7999.811503	11.342887	-0.064820	4.818512
323.556065	7999.827009	11.347891	-0.064846	4.818516
323.243977	7999.815585	11.352896	-0.064788	4.818513
323.963027	7999.805041	11.357901	-0.064922	4.818507
323.814832	7999.772675	11.362906	-0.064894	4.818498
323.604453	7999.811891	11.367911	-0.064855	4.818511
323.758975	7999.825448	11.372915	-0.064884	4.818514
323.557169	7999.893105	11.377920	-0.064846	4.818535
323.482090	7999.823923	11.382925	-0.064832	4.818515
323.161141	7999.807137	11.387930	-0.064773	4.818511
323.666657	7999.786458	11.392935	-0.064867	4.818503
323.235131	7999.895180	11.397939	-0.064786	4.818537
322.550867	7999.907223	11.402944	-0.064659	4.818543
323.584197	7999.805307	11.407949	-0.064851	4.818509
323.658589	7999.846145	11.412954	-0.064865	4.818521
323.385396	7999.875098	11.417959	-0.064814	4.818531
323.478901	7999.881563	11.422963	-0.064831	4.818532
323.360970	7999.892609	11.427968	-0.064809	4.818536
323.825340	7999.846213	11.432973	-0.064896	4.818520
323.955776	7999.795454	11.437978	-0.064920	4.818505
324.124466	7999.907824	11.442983	-0.064951	4.818537
324.238799	7999.749833	11.447987	-0.064973	4.818490
323.832524	7999.769703	11.452992	-0.064897	4.818497
323.639605	7999.828033	11.457997	-0.064861	4.818516
323.820129	7999.837733	11.463002	-0.064895	4.818518
323.644037	7999.849069	11.468007	-0.064862	4.818522
323.788612	7999.807937	11.473011	-0.064889	4.818509
323.571174	7999.783060	11.478016	-0.064848	4.818502
323.859204	7999.901184	11.483021	-0.064902	4.818536
323.327185	7999.836523	11.488026	-0.064803	4.818519
323.619549	7999.846635	11.493031	-0.064857	4.818521
323.827784	7999.821024	11.498035	-0.064896	4.818513
323.494883	7999.828213	11.503040	-0.064834	4.818516
323.921403	7999.847423	11.508045	-0.064913	4.818520
323.852080	7999.818185	11.513050	-0.064900	4.818512
323.916290	7999.781249	11.518055	-0.064912	4.818501
324.068653	7999.790582	11.523059	-0.064940	4.818503
324.054709	7999.852300	11.528064	-0.064938	4.818521
324.172028	7999.754155	11.533069	-0.064959	4.818492
324.264879	7999.940028	11.538074	-0.064977	4.818546
324.238304	7999.778097	11.543079	-0.064972	4.818498
324.189676	7999.794246	11.548083	-0.064963	4.818503
323.559916	7999.802802	11.553088	-0.064845	4.818508
324.079210	7999.798042	11.558093	-0.064942	4.818505
324.162574	7999.865230	11.563098	-0.064957	4.818525
324.290885	7999.785064	11.568103	-0.064981	4.818500
323.805485	7999.821736	11.573107	-0.064891	4.818513
324.048057	7999.791328	11.578112	-0.064936	4.818503
324.192386	7999.820490	11.583117	-0.064963	4.818511
324.341990	7999.764736	11.588122	-0.064991	4.818494
324.257042	7999.783557	11.593127	-0.064975	4.818500
324.345023	7999.901168	11.598131	-0.064991	4.818535
324.441707	7999.762882	11.603136	-0.065009	4.818493
324.371676	7999.786096	11.608141	-0.064996	4.818500
324.366066	7999.779724	11.613146	-0.064995	4.818498
324.265031	7999.895913	11.618151	-0.064976	4.818533
324.066248	7999.795735	11.623155	-0.064939	4.818504
324.151972	7999.787409	11.628160	-0.064955	4.818502
324.294107	7999.799755	11.633165	-0.064981	4.818505
324.180103	7999.781475	11.638170	-0.064960	4.818500
323.856595	7999.829705	11.643175	-0.064900	4.818515
323.954120	7999.847764	11.648179	-0.064918	4.818520
323.596381	7999.817905	11.653184	-0.064851	4.818513
323.068101	7999.979922	11.658189	-0.064753	4.818563
323.607959	7999.855822	11.663194	-0.064853	4.818524
323.868882	7999.799423	11.668199	-0.064902	4.818506
323.891926	7999.817558	11.673203	-0.064906	4.818512
323.773536	7999.809712	11.678208	-0.064884	4.818510
323.932178	7999.851652	11.683213	-0.064914	4.818522
323.601008	7999.955391	11.688218	-0.064852	4.818554
323.524483	7999.857860	11.693223	-0.064838	4.818525
323.803619	7999.882489	11.698227	-0.064889	4.818531
323.893403	7999.821755	11.703232	-0.064906	4.818513
323.842843	7999.873552	11.708237	-0.064897	4.818528
323.815648	7999.843816	11.713242	-0.064892	4.818520
323.814803	7999.800784	11.718247	-0.064891	4.818507
323.812628	7999.853213	11.723251	-0.064891	4.818522
323.967550	7999.790183	11.728256	-0.064920	4.818503
324.145556	7999.808245	11.733261	-0.064953	4.818508
323.915478	7999.802087	11.738266	-0.064910	4.818507
324.023421	7999.800347	11.743271	-0.064930	4.818506
323.607902	7999.864162	11.748275	-0.064853	4.818526
323.731380	7999.817509	11.753280	-0.064875	4.818512
323.717648	7999.856147	11.758285	-0.064873	4.818524
324.409780	7999.811679	11.763290	-0.065002	4.818508
324.365289	7999.798504	11.768295	-0.064993	4.818504
324.212516	7999.816440	11.773299	-0.064965	4.818510
324.133145	7999.798612	11.778304	-0.064950	4.818505
324.449478	7999.839466	11.783309	-0.065009	4.818516
324.037964	7999.814149	11.788314	-0.064932	4.818510
323.880896	7999.794257	11.793319	-0.064903	4.818505
324.157639	7999.806264	11.798323	-0.064954	4.818507
323.745162	7999.816609	11.803328	-0.064878	4.818512
323.851974	7999.853675	11.808333	-0.064897	4.818522
323.986909	7999.812417	11.813338	-0.064923	4.818510
324.078448	7999.804168	11.818343	-0.064940	4.818507
324.153737	7999.828231	11.823347	-0.064954	4.818514
324.453944	7999.775494	11.828352	-0.065009	4.818497
324.476226	7999.816702	11.833357	-0.065013	4.818509
324.564948	7999.872418	11.838362	-0.065030	4.818525
324.378465	7999.805975	11.843367	-0.064995	4.818506
324.345560	7999.790853	11.848371	-0.064989	4.818502
324.410674	7999.780159	11.853376	-0.065001	4.818498
324.113809	7999.843426	11.858381	-0.064946	4.818518
323.918432	7999.817787	11.863386	-0.064909	4.818512
324.294182	7999.769184	11.868391	-0.064979	4.818496
324.223910	7999.891022	11.873395	-0.064966	4.818532
324.332402	7999.807450	11.878400	-0.064986	4.818507
324.457171	7999.811176	11.883405	-0.065009	4.818507
324.437821	7999.778394	11.888410	-0.065006	4.818498
324.166175	7999.829400	11.893415	-0.064955	4.818514
324.457816	7999.829012	11.898419	-0.065009	4.818513
324.528725	7999.786917	11.903424	-0.065023	4.818500
324.476368	7999.842888	11.908429	-0.065013	4.818517
324.416856	7999.847353	11.913434	-0.065002	4.818518
324.298951	7999.865744	11.918439	-0.064980	4.818524
324.412826	7999.860934	11.923443	-0.065001	4.818522
324.617937	7999.792265	11.928448	-0.065039	4.818501
324.719938	7999.811432	11.933453	-0.065058	4.818507
324.496922	7999.808514	11.938458	-0.065016	4.818507
324.308236	7999.810241	11.943463	-0.064981	4.818508
324.465586	7999.861609	11.948467	-0.065011	4.818522
324.393238	7999.880595	11.953472	-0.064997	4.818528
323.972198	7999.875089	11.958477	-0.064919	4.818528
323.687853	7999.916486	11.963482	-0.064866	4.818542
323.659583	7999.864702	11.968487	-0.064860	4.818526
323.750548	7999.930939	11.973491	-0.064877	4.818546
323.775580	7999.867261	11.978496	-0.064882	4.818527
324.363406	7999.863399	11.983501	-0.064991	4.818523
324.184520	7999.864205	11.988506	-0.064958	4.818524
323.909960	7999.864811	11.993511	-0.064907	4.818526
324.155009	7999.890044	11.998515	-0.064952	4.818532
323.733820	7999.844666	12.003520	-0.064874	4.818520
323.604921	7999.927965	12.008525	-0.064850	4.818546
323.895088	7999.877195	12.013530	-0.064904	4.818529
324.103005	7999.859974	12.018535	-0.064942	4.818523
323.629983	7999.982842	12.023539	-0.064854	4.818562
323.241700	7999.974618	12.028544	-0.064782	4.818561
323.702690	7999.906145	12.033549	-0.064868	4.818539
323.842157	7999.872291	12.038554	-0.064894	4.818528
323.758760	7999.867001	12.043559	-0.064878	4.818527
323.891573	7999.878177	12.048563	-0.064903	4.818530
324.170936	7999.837757	12.053568	-0.064955	4.818517
324.194289	7999.842256	12.058573	-0.064959	4.818518
323.914585	7999.935126	12.063578	-0.064907	4.818546
324.016761	7999.889243	12.068583	-0.064926	4.818532
324.267407	7999.820120	12.073587	-0.064972	4.818511
323.878890	7999.841270	12.078592	-0.064900	4.818519
323.984675	7999.864683	12.083597	-0.064920	4.818525
324.338950	7999.858818	12.088602	-0.064986	4.818522
323.901076	7999.864633	12.093607	-0.064904	4.818526
323.742969	7999.909779	12.098611	-0.064875	4.818540
323.808409	7999.858170	12.103616	-0.064887	4.818524
323.900376	7999.862516	12.108621	-0.064904	4.818525
324.213072	7999.857157	12.113626	-0.064962	4.818522
324.066977	7999.845802	12.118631	-0.064935	4.818519
324.395649	7999.834356	12.123635	-0.064996	4.818515
324.192528	7999.783434	12.128640	-0.064958	4.818500
324.413740	7999.897540	12.133645	-0.064999	4.818533
324.104057	7999.843126	12.138650	-0.064942	4.818518
324.087410	7999.838709	12.143655	-0.064938	4.818517
324.060526	7999.862486	12.148659	-0.064933	4.818524
323.984137	7999.838402	12.153664	-0.064919	4.818517
323.866529	7999.876732	12.158669	-0.064897	4.818529
324.228126	7999.844732	12.163674	-0.064964	4.818518
323.843575	7999.848097	12.168679	-0.064893	4.818521
324.107205	7999.871475	12.173683	-0.064942	4.818527
323.380476	7999.942764	12.178688	-0.064807	4.818551
323.790516	7999.932381	12.183693	-0.064883	4.818546
324.266246	7999.844166	12.188698	-0.064971	4.818518
323.868369	7999.874636	12.193703	-0.064897	4.818529
323.935513	7999.875511	12.198707	-0.064910	4.818529
324.560872	7999.776660	12.203712	-0.065026	4.818497
324.305903	7999.831032	12.208717	-0.064978	4.818514
324.061974	7999.829939	12.213722	-0.064933	4.818515
323.723894	7999.849650	12.218727	-0.064870	4.818522
323.822647	7999.921235	12.223731	-0.064888	4.818543
324.033234	7999.814866	12.228736	-0.064928	4.818510
323.940949	7999.871363	12.233741	-0.064910	4.818527
323.973544	7999.847654	12.238746	-0.064916	4.818520
324.119047	7999.796043	12.243751	-0.064943	4.818504
324.134355	7999.935786	12.248755	-0.064946	4.818546
323.944903	7999.849369	12.253760	-0.064911	4.818521
323.822547	7999.949541	12.258765	-0.064888	4.818551
323.881687	7999.878964	12.263770	-0.064899	4.818530
323.709393	7999.890349	12.268775	-0.064867	4.818534
324.330415	7999.848100	12.273779	-0.064982	4.818519
324.021921	7999.828327	12.278784	-0.064925	4.818514
323.590977	7999.920269	12.283789	-0.064845	4.818543
324.018494	7999.849260	12.288794	-0.064924	4.818521
324.038645	7999.877849	12.293799	-0.064928	4.818529
323.645153	7999.988117	12.298803	-0.064855	4.818563
323.946304	7999.882932	12.303808	-0.064911	4.818531
324.684521	7999.852707	12.308813	-0.065048	4.818519
324.471394	7999.823687	12.313818	-0.065008	4.818511
324.206789	7999.824423	12.318823	-0.064959	4.818512
324.013007	7999.912120	12.323827	-0.064923	4.818539
323.944476	7999.866105	12.328832	-0.064910	4.818526
324.219722	7999.879142	12.333837	-0.064961	4.818529
323.861554	7999.919574	12.338842	-0.064895	4.818542
323.691695	7999.916302	12.343847	-0.064863	4.818542
324.273133	7999.925997	12.348851	-0.064971	4.818542
323.967358	7999.885274	12.353856	-0.064914	4.818531
323.695931	7999.903758	12.358861	-0.064864	4.818538
323.980227	7999.875993	12.363866	-0.064917	4.818529
324.165000	7999.832240	12.368871	-0.064951	4.818515
324.211252	7999.873761	12.373875	-0.064959	4.818527
324.153057	7999.823684	12.378880	-0.064949	4.818512
324.583862	7999.846099	12.383885	-0.065029	4.818517
324.068188	7999.864537	12.388890	-0.064933	4.818525
324.418734	7999.846033	12.393895	-0.064998	4.818518
324.304353	7999.898045	12.398899	-0.064977	4.818534
324.407898	7999.828048	12.403904	-0.064996	4.818513
324.286144	7999.868423	12.408909	-0.064973	4.818525
324.252324	7999.867978	12.413914	-0.064967	4.818525
324.230662	7999.866642	12.418919	-0.064963	4.818525
324.595967	7999.823150	12.423923	-0.065031	4.818511
324.507798	7999.818846	12.428928	-0.065014	4.818510
324.536511	7999.893714	12.433933	-0.065019	4.818532
324.473651	7999.926464	12.438938	-0.065008	4.818542
323.925913	7999.959172	12.443943	-0.064906	4.818554
324.290424	7999.970229	12.448947	-0.064974	4.818556
323.567144	7999.969166	12.453952	-0.064839	4.818558
324.002894	7999.888822	12.458957	-0.064920	4.818532
323.983445	7999.899057	12.463962	-0.064916	4.818536
323.567756	7999.943983	12.468967	-0.064839	4.818551
323.759100	7999.953825	12.473971	-0.064874	4.818553
324.310943	7999.856113	12.478976	-0.064977	4.818522
323.994399	7999.912827	12.483981	-0.064918	4.818540
324.769991	7999.803351	12.488986	-0.065062	4.818504
324.486717	7999.845811	12.493991	-0.065010	4.818518
324.509590	7999.890174	12.498995	-0.065014	4.818531
324.216217	7999.846466	12.504000	-0.064959	4.818519
325.151898	7999.836661	12.509005	-0.065133	4.818512
324.831588	7999.869193	12.514010	-0.065074	4.818523
324.127525	7999.916644	12.519015	-0.064943	4.818540
324.297108	7999.886332	12.524019	-0.064974	4.818531
324.498623	7999.827059	12.529024	-0.065012	4.818512
324.510178	7999.856585	12.534029	-0.065014	4.818521
324.260386	7999.823939	12.539034	-0.064967	4.818512
323.733711	7999.871612	12.544039	-0.064869	4.818528
324.236473	7999.844604	12.549043	-0.064963	4.818518
324.340158	7999.847006	12.554048	-0.064982	4.818519
324.619063	7999.840156	12.559053	-0.065034	4.818516
324.626706	7999.857041	12.564058	-0.065035	4.818521
324.639705	7999.825730	12.569063	-0.065037	4.818511
324.845536	7999.828418	12.574067	-0.065076	4.818511
324.375426	7999.845353	12.579072	-0.064988	4.818518
324.757305	7999.849292	12.584077	-0.065059	4.818518
324.487743	7999.896128	12.589082	-0.065009	4.818533
324.124674	7999.892429	12.594087	-0.064941	4.818533
324.127627	7999.901907	12.599091	-0.064942	4.818536
324.429069	7999.840792	12.604096	-0.064998	4.818517
324.237171	7999.884447	12.609101	-0.064962	4.818530
324.204925	7999.935434	12.614106	-0.064956	4.818546
324.197626	7999.865038	12.619111	-0.064955	4.818525
324.000900	7999.955844	12.624115	-0.064918	4.818552
323.590067	8000.042803	12.629120	-0.064842	4.818580
323.955325	7999.922717	12.634125	-0.064910	4.818543
324.101533	7999.946658	12.639130	-0.064937	4.818549
324.484248	7999.861424	12.644135	-0.065008	4.818522
324.741328	7999.870028	12.649139	-0.065056	4.818524
324.784265	7999.803436	12.654144	-0.065064	4.818504
324.929320	7999.834707	12.659149	-0.065091	4.818513
324.829208	7999.807165	12.664154	-0.065072	4.818505
324.851089	7999.798004	12.669159	-0.065076	4.818502
324.712558	7999.848652	12.674163	-0.065050	4.818518
324.586518	7999.826017	12.679168	-0.065027	4.818512
324.581356	7999.856374	12.684173	-0.065026	4.818521
324.542941	7999.828589	12.689178	-0.065018	4.818512
324.316616	7999.872842	12.694183	-0.064976	4.818526
324.087093	7999.947482	12.699187	-0.064934	4.818550
324.113276	7999.899557	12.704192	-0.064938	4.818535
324.012207	8000.003155	12.709197	-0.064920	4.818566
323.862085	7999.989648	12.714202	-0.064892	4.818563
324.210778	7999.909215	12.719207	-0.064956	4.818538
324.090402	7999.960100	12.724211	-0.064934	4.818553
324.358466	7999.906943	12.729216	-0.064984	4.818536
324.295590	7999.876740	12.734221	-0.064972	4.818528
323.956348	7999.981422	12.739226	-0.064909	4.818560
324.478384	7999.844498	12.744231	-0.065006	4.818517
324.125730	7999.956350	12.749235	-0.064940	4.818552
323.649371	7999.939628	12.754240	-0.064852	4.818549
323.953507	7999.924714	12.759245	-0.064908	4.818543
324.386122	7999.864265	12.764250	-0.064989	4.818524
324.217614	7999.849468	12.769255	-0.064957	4.818520
324.352635	7999.918381	12.774259	-0.064982	4.818540
324.171567	7999.861451	12.779264	-0.064948	4.818524
323.766285	7999.949532	12.784269	-0.064873	4.818551
323.968984	7999.903914	12.789274	-0.064911	4.818537
324.147413	7999.906243	12.794279	-0.064944	4.818537
324.714983	7999.888478	12.799283	-0.065050	4.818530
324.492968	7999.868784	12.804288	-0.065008	4.818525
323.976627	7999.928133	12.809293	-0.064912	4.818544
324.099010	8000.000028	12.814298	-0.064935	4.818565
323.690227	8000.010420	12.819303	-0.064859	4.818570
323.770659	8000.061830	12.824307	-0.064874	4.818585
324.167300	7999.920121	12.829312	-0.064947	4.818541
324.416274	7999.976883	12.834317	-0.064994	4.818557
323.877759	8000.039089	12.839322	-0.064893	4.818578
323.934016	7999.939096	12.844327	-0.064904	4.818548
323.985933	7999.971248	12.849331	-0.064913	4.818557
323.847255	7999.944251	12.854336	-0.064887	4.818550
324.139181	7999.899800	12.859341	-0.064942	4.818535
323.643657	7999.984602	12.864346	-0.064850	4.818562
323.690069	7999.965271	12.869351	-0.064858	4.818556
323.855653	7999.954841	12.874355	-0.064889	4.818553
323.820859	7999.955432	12.879360	-0.064882	4.818553
324.468992	7999.869471	12.884365	-0.065003	4.818525
324.240453	7999.939926	12.889370	-0.064960	4.818547
323.956478	7999.905784	12.894375	-0.064907	4.818538
324.102016	7999.986375	12.899379	-0.064935	4.818561
324.110373	7999.941364	12.904384	-0.064936	4.818548
323.773453	8000.011452	12.909389	-0.064873	4.818570
323.942687	8000.028350	12.914394	-0.064905	4.818574
324.168462	7999.916933	12.919399	-0.064947	4.818540
324.190613	7999.972828	12.924403	-0.064951	4.818557
323.721852	8000.016011	12.929408	-0.064864	4.818571
323.638563	8000.002329	12.934413	-0.064848	4.818568
323.811372	7999.971010	12.939418	-0.064880	4.818558
323.669683	7999.913547	12.944423	-0.064854	4.818541
323.894553	7999.940614	12.949427	-0.064895	4.818548
324.288124	7999.897491	12.954432	-0.064969	4.818534
324.167026	7999.900102	12.959437	-0.064946	4.818535
324.109025	7999.944457	12.964442	-0.064935	4.818549
324.040349	7999.909982	12.969447	-0.064922	4.818539
324.109774	7999.954953	12.974451	-0.064935	4.818552
324.073168	7999.882075	12.979456	-0.064928	4.818530
324.598482	7999.856413	12.984461	-0.065026	4.818521
323.981535	8000.014123	12.989466	-0.064911	4.818570
323.860635	7999.952734	12.994471	-0.064889	4.818552
324.644197	7999.938841	12.999475	-0.065035	4.818545
323.938339	8000.005155	13.004480	-0.064903	4.818567
323.590923	8000.042580	13.009485	-0.064838	4.818580
323.938538	8000.015644	13.014490	-0.064903	4.818571
323.664382	7999.982679	13.019495	-0.064852	4.818562
324.445307	7999.921536	13.024499	-0.064997	4.818541
324.369821	7999.863888	13.029504	-0.064983	4.818524
324.174454	7999.917990	13.034509	-0.064947	4.818541
324.573022	7999.877031	13.039514	-0.065021	4.818527
324.753414	7999.857352	13.044519	-0.065055	4.818520
324.872508	7999.888285	13.049523	-0.065077	4.818529
324.799416	7999.865292	13.054528	-0.065063	4.818522
324.505636	7999.892925	13.059533	-0.065008	4.818532
324.375348	7999.976206	13.064538	-0.064984	4.818557
324.201230	7999.902580	13.069543	-0.064951	4.818536
324.382683	7999.916490	13.074547	-0.064985	4.818539
324.649957	7999.857027	13.079552	-0.065035	4.818521
324.468269	7999.872486	13.084557	-0.065001	4.818526
324.415436	7999.907466	13.089562	-0.064991	4.818536
324.097139	7999.888613	13.094567	-0.064932	4.818532
324.144650	7999.944840	13.099571	-0.064941	4.818549
324.116054	7999.896199	13.104576	-0.064935	4.818534
324.244318	7999.882134	13.109581	-0.064959	4.818530
324.237336	7999.908270	13.114586	-0.064958	4.818537
323.564264	8000.008589	13.119591	-0.064833	4.818570
324.401777	7999.879986	13.124595	-0.064988	4.818528
324.660512	7999.842445	13.129600	-0.065036	4.818516
324.165285	7999.947186	13.134605	-0.064944	4.818549
323.954033	8000.033606	13.139610	-0.064905	4.818576
323.945873	7999.954805	13.144615	-0.064903	4.818552
324.149461	7999.939626	13.149619	-0.064941	4.818547
324.044731	7999.981272	13.154624	-0.064922	4.818560
323.909336	8000.026714	13.159629	-0.064896	4.818574
323.869614	8000.035635	13.164634	-0.064889	4.818577
323.695579	8000.028111	13.169639	-0.064857	4.818575
323.786427	8000.082805	13.174643	-0.064873	4.818591
323.776443	7999.986144	13.179648	-0.064871	4.818562
324.344993	7999.905437	13.184653	-0.064977	4.818536
324.563665	7999.914588	13.189658	-0.065018	4.818538
324.120979	7999.925586	13.194663	-0.064935	4.818543
324.151505	7999.969000	13.199667	-0.064941	4.818556
324.044994	8000.003278	13.204672	-0.064921	4.818566
324.026106	8000.017717	13.209677	-0.064918	4.818571
324.118145	8000.031508	13.214682	-0.064935	4.818575
324.657924	7999.900064	13.219687	-0.065035	4.818533
324.570948	7999.944040	13.224691	-0.065019	4.818547
324.409551	7999.933533	13.229696	-0.064989	4.818544
324.442607	7999.972784	13.234701	-0.064995	4.818556
325.160707	7999.859409	13.239706	-0.065129	4.818519
324.629996	7999.884994	13.244711	-0.065030	4.818529
324.594091	8000.000986	13.249715	-0.065023	4.818564
324.834701	7999.902353	13.254720	-0.065068	4.818533
324.594455	7999.904455	13.259725	-0.065023	4.818535
324.422214	7999.982991	13.264730	-0.064991	4.818559
324.182347	8000.003985	13.269735	-0.064946	4.818566
324.067505	7999.978348	13.274739	-0.064925	4.818559
324.164340	7999.924002	13.279744	-0.064943	4.818542
323.873782	7999.936989	13.284749	-0.064889	4.818547
324.386297	7999.922700	13.289754	-0.064984	4.818541
324.374442	7999.881622	13.294759	-0.064982	4.818529
324.150780	7999.965781	13.299763	-0.064940	4.818555
323.926816	8000.009016	13.304768	-0.064898	4.818569
324.000329	8000.001580	13.309773	-0.064912	4.818566
323.689534	8000.069911	13.314778	-0.064854	4.818588
324.233876	7999.892360	13.319783	-0.064955	4.818533
324.513640	7999.857193	13.324787	-0.065007	4.818521
324.708061	7999.818811	13.329792	-0.065044	4.818509
324.250573	7999.934538	13.334797	-0.064958	4.818545
324.191745	7999.975735	13.339802	-0.064947	4.818558
324.579241	7999.856989	13.344807	-0.065019	4.818521
324.095295	7999.994403	13.349811	-0.064929	4.818564
324.333837	7999.917777	13.354816	-0.064974	4.818540
324.452743	7999.927723	13.359821	-0.064996	4.818542
324.619769	7999.886885	13.364826	-0.065027	4.818530
324.240487	7999.934385	13.369831	-0.064956	4.818545
324.806064	7999.894560	13.374835	-0.065061	4.818531
325.048832	7999.935504	13.379840	-0.065107	4.818542
325.113585	7999.848211	13.384845	-0.065119	4.818516
325.166079	7999.887717	13.389850	-0.065128	4.818528
324.425742	7999.947283	13.394855	-0.064990	4.818548
325.047953	7999.894560	13.399859	-0.065106	4.818530
325.215225	7999.835888	13.404864	-0.065137	4.818512
325.075674	7999.848750	13.409869	-0.065111	4.818517
325.471577	7999.813003	13.414874	-0.065185	4.818504
325.093702	7999.817502	13.419879	-0.065115	4.818507
325.381246	7999.827554	13.424883	-0.065168	4.818509
325.436477	7999.773713	13.429888	-0.065178	4.818493
325.325535	7999.816327	13.434893	-0.065158	4.818506
325.114687	7999.839798	13.439898	-0.065118	4.818514
325.283614	7999.794788	13.444903	-0.065150	4.818500
325.061046	7999.835943	13.449907	-0.065108	4.818513
325.191622	7999.805121	13.454912	-0.065132	4.818503
325.444271	7999.867179	13.459917	-0.065180	4.818521
325.448797	7999.831561	13.464922	-0.065180	4.818510
325.505638	7999.796627	13.469927	-0.065191	4.818499
325.813859	7999.812196	13.474931	-0.065248	4.818503
325.608038	7999.784319	13.479936	-0.065210	4.818495
325.672143	7999.799844	13.484941	-0.065222	4.818500
325.606942	7999.805284	13.489946	-0.065209	4.818502
325.322184	7999.815197	13.494951	-0.065156	4.818506
325.106115	7999.826009	13.499955	-0.065116	4.818510
325.051981	7999.843135	13.504960	-0.065106	4.818515
325.428780	7999.816582	13.509965	-0.065176	4.818506
325.164362	7999.830958	13.514970	-0.065127	4.818511
325.262447	7999.823844	13.519975	-0.065145	4.818508
325.483484	7999.830928	13.524979	-0.065186	4.818510
325.545788	7999.889449	13.529984	-0.065198	4.818527
325.490582	7999.816325	13.534989	-0.065187	4.818505
324.967249	7999.912305	13.539994	-0.065090	4.818536
325.202612	7999.815701	13.544999	-0.065134	4.818506
325.271774	7999.845981	13.550003	-0.065147	4.818515
324.913302	7999.868571	13.555008	-0.065080	4.818523
324.997083	7999.853925	13.560013	-0.065095	4.818518
324.885436	7999.873447	13.565018	-0.065075	4.818525
324.851089	7999.843616	13.570023	-0.065068	4.818516
325.216078	7999.845238	13.575027	-0.065136	4.818515
325.091177	7999.834158	13.580032	-0.065113	4.818512
324.898789	7999.883052	13.585037	-0.065077	4.818527
325.342922	7999.869970	13.590042	-0.065159	4.818522
324.997985	7999.865457	13.595047	-0.065095	4.818522
325.104259	7999.868942	13.600051	-0.065115	4.818522
325.002754	7999.835085	13.605056	-0.065096	4.818513
324.885101	7999.863972	13.610061	-0.065074	4.818522
325.345240	7999.836409	13.615066	-0.065160	4.818512
324.941801	7999.839525	13.620071	-0.065085	4.818514
324.689320	7999.886584	13.625075	-0.065037	4.818529
325.158799	7999.840258	13.630080	-0.065125	4.818514
324.951899	7999.858534	13.635085	-0.065086	4.818520
325.301831	7999.843171	13.640090	-0.065151	4.818514
325.252438	7999.838325	13.645095	-0.065142	4.818513
325.098570	7999.877231	13.650099	-0.065113	4.818525
324.705347	7999.865791	13.655104	-0.065040	4.818523
324.604905	8000.014515	13.660109	-0.065022	4.818568
325.034040	7999.960317	13.665114	-0.065101	4.818550
325.108260	7999.840622	13.670119	-0.065115	4.818514
324.987330	7999.899893	13.675123	-0.065093	4.818532
325.034433	7999.855389	13.680128	-0.065101	4.818519
324.862631	7999.883567	13.685133	-0.065069	4.818528
324.900393	7999.850482	13.690138	-0.065076	4.818518
324.702897	7999.854193	13.695143	-0.065039	4.818520
324.788280	7999.898324	13.700147	-0.065055	4.818532
324.641238	7999.933122	13.705152	-0.065028	4.818543
324.552956	7999.916226	13.710157	-0.065011	4.818539
324.705835	7999.920320	13.715162	-0.065040	4.818539
324.619515	7999.859383	13.720167	-0.065024	4.818522
324.413637	7999.937479	13.725171	-0.064985	4.818546
324.769321	7999.858187	13.730176	-0.065051	4.818521
324.999692	7999.810833	13.735181	-0.065094	4.818506
324.557269	7999.888984	13.740186	-0.065012	4.818531
324.957022	7999.845943	13.745191	-0.065086	4.818516
325.257612	7999.848821	13.750195	-0.065142	4.818516
325.140038	7999.825246	13.755200	-0.065120	4.818509
325.243849	7999.828699	13.760205	-0.065140	4.818510
324.504501	7999.912411	13.765210	-0.065002	4.818538
324.886823	7999.819828	13.770215	-0.065073	4.818509
324.693433	7999.945303	13.775219	-0.065037	4.818547
324.581320	7999.880880	13.780224	-0.065016	4.818528
324.370719	7999.908552	13.785229	-0.064977	4.818537
324.396338	7999.939311	13.790234	-0.064982	4.818546
324.562673	7999.916301	13.795239	-0.065012	4.818539
325.229630	7999.931314	13.800243	-0.065137	4.818541
324.955526	7999.823852	13.805248	-0.065085	4.818510
325.038800	7999.886843	13.810253	-0.065101	4.818528
324.966697	7999.880651	13.815258	-0.065087	4.818526
325.192438	7999.831137	13.820263	-0.065129	4.818511
324.867204	7999.878295	13.825267	-0.065069	4.818526
325.062112	7999.843067	13.830272	-0.065105	4.818515
324.991376	7999.843189	13.835277	-0.065092	4.818515
325.195540	7999.835363	13.840282	-0.065130	4.818512
325.077240	7999.817025	13.845287	-0.065108	4.818507
325.150078	7999.845254	13.850291	-0.065121	4.818515
324.759704	7999.917791	13.855296	-0.065049	4.818538
325.296683	7999.837722	13.860301	-0.065148	4.818512
325.507566	7999.826836	13.865306	-0.065188	4.818508
325.210810	7999.858627	13.870311	-0.065132	4.818519
324.969398	7999.932062	13.875315	-0.065087	4.818542
325.202024	7999.876343	13.880320	-0.065131	4.818524
325.101482	7999.911749	13.885325	-0.065112	4.818535
325.506002	7999.846736	13.890330	-0.065187	4.818514
325.255825	7999.766867	13.895335	-0.065141	4.818492
325.339769	7999.840359	13.900339	-0.065156	4.818513
324.929744	7999.846537	13.905344	-0.065080	4.818517
325.189677	7999.818455	13.910349	-0.065128	4.818507
324.632100	7999.907692	13.915354	-0.065024	4.818536
324.920794	7999.828573	13.920359	-0.065078	4.818511
324.642020	7999.947686	13.925363	-0.065026	4.818548
324.614970	7999.899065	13.930368	-0.065021	4.818533
324.589666	7999.935454	13.935373	-0.065016	4.818544
324.804210	7999.903631	13.940378	-0.065056	4.818534
325.070598	7999.857797	13.945383	-0.065106	4.818519
324.863190	7999.946366	13.950387	-0.065067	4.818546
324.558792	7999.916152	13.955392	-0.065010	4.818539
324.479030	7999.920352	13.960397	-0.064995	4.818540
325.073141	7999.887196	13.965402	-0.065106	4.818528
324.485451	7999.904691	13.970407	-0.064997	4.818536
324.451840	7999.971400	13.975411	-0.064990	4.818556
324.014164	8000.010792	13.980416	-0.064909	4.818569
324.235996	7999.992704	13.985421	-0.064950	4.818563
324.511862	7999.978470	13.990426	-0.065001	4.818557
324.552458	7999.899256	13.995431	-0.065009	4.818534
324.736189	7999.898508	14.000435	-0.065043	4.818533
324.656537	7999.863888	14.005440	-0.065028	4.818523
324.947629	7999.825721	14.010445	-0.065082	4.818510
324.933620	7999.875898	14.015450	-0.065080	4.818525
324.463462	7999.891782	14.020455	-0.064992	4.818532
324.444213	7999.927201	14.025459	-0.064988	4.818542
324.533034	7999.954590	14.030464	-0.065005	4.818550
324.494856	8000.001304	14.035469	-0.064998	4.818564
324.439852	7999.975400	14.040474	-0.064987	4.818557
324.909750	7999.921734	14.045479	-0.065075	4.818539
324.654610	7999.949872	14.050483	-0.065027	4.818548
325.019465	7999.900079	14.055488	-0.065095	4.818532
325.361556	7999.819561	14.060493	-0.065159	4.818507
325.369372	7999.846940	14.065498	-0.065160	4.818515
324.163323	7999.984357	14.070503	-0.064936	4.818561
324.647197	7999.964449	14.075507	-0.065026	4.818553
324.348681	7999.915426	14.080512	-0.064970	4.818539
324.748278	7999.879727	14.085517	-0.065044	4.818527
325.091187	7999.880011	14.090522	-0.065108	4.818526
325.001375	7999.873587	14.095527	-0.065091	4.818524
324.773985	7999.885300	14.100531	-0.065049	4.818529
324.803973	7999.887788	14.105536	-0.065055	4.818529
324.682889	7999.878857	14.110541	-0.065032	4.818527
324.922455	7999.884084	14.115546	-0.065077	4.818528
324.869114	7999.891778	14.120551	-0.065067	4.818530
324.911576	7999.900724	14.125555	-0.065075	4.818533
325.363085	7999.868852	14.130560	-0.065159	4.818522
325.220044	7999.860683	14.135565	-0.065132	4.818520
325.462505	7999.839718	14.140570	-0.065177	4.818512
325.177689	7999.828646	14.145575	-0.065124	4.818510
325.392641	7999.852438	14.150579	-0.065164	4.818517
325.505454	7999.859157	14.155584	-0.065185	4.818518
324.743304	7999.907945	14.160589	-0.065043	4.818536
325.092022	7999.917748	14.165594	-0.065108	4.818537
325.079540	7999.853578	14.170599	-0.065105	4.818518
325.205729	7999.863619	14.175603	-0.065129	4.818521
324.870198	7999.895952	14.180608	-0.065066	4.818531
324.924982	7999.865188	14.185613	-0.065076	4.818522
325.247129	7999.891431	14.190618	-0.065136	4.818529
325.414085	7999.863184	14.195623	-0.065167	4.818520
325.319944	7999.866146	14.200627	-0.065150	4.818521
325.294033	7999.896233	14.205632	-0.065145	4.818530
324.846165	7999.913456	14.210637	-0.065062	4.818537
324.783518	7999.997622	14.215642	-0.065050	4.818562
324.942618	7999.908416	14.220647	-0.065079	4.818535
324.881134	7999.914953	14.225651	-0.065068	4.818537
325.016865	7999.870559	14.230656	-0.065093	4.818523
325.092777	7999.873647	14.235661	-0.065107	4.818524
324.851202	7999.918750	14.240666	-0.065062	4.818538
324.012926	8000.003268	14.245671	-0.064906	4.818567
323.955728	8000.027698	14.250675	-0.064896	4.818574
324.424423	8000.018084	14.255680	-0.064983	4.818570
324.174828	8000.011670	14.260685	-0.064936	4.818569
324.392718	7999.981989	14.265690	-0.064977	4.818559
324.472106	7999.965187	14.270695	-0.064991	4.818554
324.529165	8000.002653	14.275699	-0.065002	4.818565
324.170597	8000.045178	14.280704	-0.064935	4.818579
324.559099	7999.975759	14.285709	-0.065008	4.818556
324.463483	8000.033263	14.290714	-0.064990	4.818574
324.502607	7999.925700	14.295719	-0.064997	4.818542
324.836704	7999.943705	14.300723	-0.065059	4.818546
324.888663	7999.881427	14.305728	-0.065069	4.818527
324.565976	7999.904485	14.310733	-0.065009	4.818535
324.608361	7999.935464	14.315738	-0.065016	4.818544
324.804738	7999.869828	14.320743	-0.065053	4.818524
324.575428	7999.950766	14.325747	-0.065010	4.818549
324.655254	7999.936068	14.330752	-0.065025	4.818544
325.013097	7999.861001	14.335757	-0.065092	4.818521
324.929933	7999.923915	14.340762	-0.065076	4.818540
324.866678	7999.867475	14.345767	-0.065064	4.818523
324.909440	7999.648742	14.350771	-0.065072	4.818458

324.657347	7996.523280	14.355776	-0.065023	4.817529
324.251519	7990.921499	14.360781	-0.064944	4.815863
324.301231	7984.128378	14.365786	-0.064948	4.813840
324.242131	7976.851638	14.370791	-0.064933	4.811672
324.180556	7969.204311	14.375795	-0.064916	4.809393
324.221681	7961.428952	14.380800	-0.064919	4.807074
324.441043	7953.426163	14.385805	-0.064954	4.804686
324.777722	7945.572964	14.390810	-0.065012	4.802341
324.786260	7937.497064	14.395815	-0.065008	4.799929
324.342107	7929.618565	14.400819	-0.064920	4.797577
324.443092	7921.619684	14.405824	-0.064934	4.795185
324.618479	7913.553572	14.410829	-0.064961	4.792772
324.484961	7905.585137	14.415834	-0.064931	4.790388
324.158541	7897.587409	14.420839	-0.064865	4.787995
324.457980	7889.580524	14.425843	-0.064916	4.785596
323.944380	7881.648403	14.430848	-0.064815	4.783220
323.659455	7873.651931	14.435853	-0.064756	4.780823
323.343067	7865.699856	14.440858	-0.064692	4.778439
323.569591	7857.559520	14.445863	-0.064729	4.775995
323.555550	7849.549888	14.450867	-0.064721	4.773590
323.846131	7841.581403	14.455872	-0.064770	4.771195
323.510013	7833.547811	14.460877	-0.064702	4.768781
323.919365	7825.530210	14.465882	-0.064773	4.766368
324.021020	7817.474439	14.470887	-0.064787	4.763944
324.099942	7809.581173	14.475891	-0.064796	4.761568
323.682091	7801.538496	14.480896	-0.064713	4.759146
323.595072	7793.608397	14.485901	-0.064692	4.756757
323.816838	7785.539832	14.490906	-0.064728	4.754323
323.447706	7777.552516	14.495911	-0.064654	4.751915
322.868909	7769.594718	14.500915	-0.064541	4.749514
323.414703	7761.487105	14.505920	-0.064637	4.747065
323.419979	7753.437488	14.510925	-0.064633	4.744633
323.422175	7745.564419	14.515930	-0.064628	4.742253
323.518932	7737.500892	14.520935	-0.064641	4.739814
323.451370	7729.558005	14.525939	-0.064623	4.737411
323.790142	7721.495979	14.530944	-0.064681	4.734969
323.258481	7713.559389	14.535949	-0.064576	4.732566
323.413496	7705.535344	14.540954	-0.064600	4.730134
323.459250	7697.507541	14.545959	-0.064603	4.727700
323.254404	7689.476298	14.550963	-0.064560	4.725264
323.142083	7681.596829	14.555968	-0.064534	4.722872
322.925077	7673.544083	14.560973	-0.064488	4.720427
323.370826	7665.554369	14.565978	-0.064566	4.717999
322.808148	7657.542224	14.570983	-0.064456	4.715564
323.103496	7649.506566	14.575987	-0.064506	4.713120
323.004303	7641.544008	14.580992	-0.064482	4.710697
323.173963	7633.527267	14.585997	-0.064508	4.708255
323.279375	7625.483631	14.591002	-0.064522	4.705805
323.123975	7617.494362	14.596007	-0.064488	4.703370
322.913823	7609.564370	14.601011	-0.064444	4.700952
323.051759	7601.539487	14.606016	-0.064464	4.698504
322.897799	7593.550518	14.611021	-0.064430	4.696065
322.766140	7585.552550	14.616026	-0.064401	4.693622
322.590308	7577.524973	14.621031	-0.064363	4.691169
322.488634	7569.515139	14.626035	-0.064338	4.688720
322.132804	7561.567072	14.631040	-0.064267	4.686289
322.156550	7553.420180	14.636045	-0.064266	4.683796
322.455787	7545.553385	14.641050	-0.064317	4.681387
321.924715	7537.538210	14.646055	-0.064212	4.678931
322.231396	7529.565516	14.651059	-0.064264	4.676487
322.254231	7521.469257	14.656064	-0.064263	4.674004
321.702807	7513.557600	14.661069	-0.064155	4.671576
322.229806	7505.415620	14.666074	-0.064248	4.669076
321.988229	7497.451865	14.671079	-0.064198	4.666630
321.951917	7489.398094	14.676083	-0.064186	4.664154
321.581693	7481.572750	14.681088	-0.064112	4.661748
322.093201	7473.343078	14.686093	-0.064202	4.659215
321.767445	7465.530220	14.691098	-0.064136	4.656810
321.580878	7457.433741	14.696103	-0.064096	4.654316
321.469228	7449.526999	14.701107	-0.064070	4.651880
321.466551	7441.421955	14.706112	-0.064064	4.649380
321.467541	7433.489216	14.711117	-0.064059	4.646933
321.667417	7425.387589	14.716122	-0.064091	4.644432
321.175839	7417.518362	14.721127	-0.063994	4.642002
321.702707	7409.436044	14.726131	-0.064087	4.639505
321.279478	7401.560133	14.731136	-0.064003	4.637069
321.656611	7393.428933	14.736141	-0.064068	4.634554
321.502501	7385.475416	14.741146	-0.064034	4.632093
321.260508	7377.465897	14.746151	-0.063984	4.629612
321.468865	7369.433591	14.751155	-0.064017	4.627124
321.755251	7361.345944	14.756160	-0.064065	4.624617
321.539770	7353.433940	14.761165	-0.064020	4.622163
321.147636	7345.491519	14.766170	-0.063942	4.619697
320.678351	7337.495428	14.771175	-0.063849	4.617214
320.902336	7329.459436	14.776179	-0.063885	4.614718
320.710266	7321.490364	14.781184	-0.063844	4.612240
320.407040	7313.400609	14.786189	-0.063783	4.609724
320.793821	7305.417120	14.791194	-0.063849	4.607240
320.336497	7297.447141	14.796199	-0.063759	4.604758
320.453532	7289.443197	14.801203	-0.063775	4.602265
320.680230	7281.372983	14.806208	-0.063812	4.599750
320.768794	7273.434834	14.811213	-0.063824	4.597275
320.729404	7265.369500	14.816218	-0.063811	4.594758
320.981847	7257.339166	14.821223	-0.063853	4.592251
320.889685	7249.358852	14.826227	-0.063830	4.589758
320.664878	7241.446535	14.831232	-0.063783	4.587285
320.598580	7233.367035	14.836237	-0.063766	4.584758
320.308820	7225.486820	14.841242	-0.063707	4.582292
320.090209	7217.376253	14.846247	-0.063660	4.579753
320.586179	7209.409424	14.851251	-0.063748	4.577258
320.225509	7201.339587	14.856256	-0.063675	4.574729
320.261175	7193.402193	14.861261	-0.063677	4.572240
320.541176	7185.350100	14.866266	-0.063723	4.569714
319.472342	7177.414011	14.871271	-0.063519	4.567221
320.368919	7169.280025	14.876275	-0.063681	4.564668
320.048088	7161.407353	14.881280	-0.063616	4.562193
319.987767	7153.341604	14.886285	-0.063599	4.559657
320.259627	7145.384984	14.891290	-0.063645	4.557154
320.124350	7137.304941	14.896295	-0.063614	4.554610
320.387304	7129.325377	14.901299	-0.063658	4.552098
319.880217	7121.381206	14.906304	-0.063558	4.549593
319.970942	7113.364334	14.911309	-0.063570	4.547065
319.612768	7105.344869	14.916314	-0.063498	4.544534
319.387827	7097.366422	14.921319	-0.063451	4.542015
319.278115	7089.340077	14.926323	-0.063425	4.539480
319.835896	7081.340780	14.931328	-0.063524	4.536953
319.645076	7073.291547	14.936333	-0.063483	4.534408
319.921136	7065.354916	14.941338	-0.063529	4.531898
319.766989	7057.262120	14.946343	-0.063495	4.529335
319.678151	7049.357599	14.951347	-0.063473	4.526832
319.367488	7041.304134	14.956352	-0.063410	4.524278
319.280920	7033.357365	14.961357	-0.063389	4.521758
319.620984	7025.300392	14.966362	-0.063447	4.519203
318.701725	7017.444240	14.971367	-0.063271	4.516706
319.051412	7009.302813	14.976371	-0.063330	4.514122
318.776939	7001.366331	14.981376	-0.063274	4.511598
318.736877	6993.246244	14.986381	-0.063261	4.509016
319.026094	6985.232987	14.991386	-0.063310	4.506468
319.109578	6977.226565	14.996391	-0.063320	4.503919
319.524187	6969.308901	15.001395	-0.063392	4.501399
319.278064	6961.274232	15.006400	-0.063341	4.498837
318.674753	6953.322038	15.011405	-0.063223	4.496299
319.058641	6945.274227	15.016410	-0.063290	4.493733
319.225243	6937.240467	15.021415	-0.063315	4.491169
318.621749	6929.280745	15.026419	-0.063198	4.488624
318.599921	6921.257644	15.031424	-0.063188	4.486059
318.636471	6913.232520	15.036429	-0.063190	4.483493
318.963406	6905.244169	15.041434	-0.063246	4.480938
318.504074	6897.256354	15.046439	-0.063155	4.478379
318.264038	6889.301439	15.051443	-0.063105	4.475829
318.340335	6881.260061	15.056448	-0.063114	4.473252
318.436210	6873.254158	15.061453	-0.063126	4.470685
318.625051	6865.221334	15.066458	-0.063156	4.468108
318.272635	6857.240837	15.071463	-0.063085	4.465544
318.168464	6849.240997	15.076467	-0.063061	4.462973
318.442383	6841.219756	15.081472	-0.063106	4.460396
318.405156	6833.225244	15.086477	-0.063094	4.457824
318.153892	6825.252237	15.091482	-0.063042	4.455257
317.983687	6817.278794	15.096487	-0.063005	4.452689
318.516774	6809.156543	15.101491	-0.063099	4.450074
317.846755	6801.288474	15.106496	-0.062969	4.447534
317.778476	6793.168731	15.111501	-0.062951	4.444915
317.947985	6785.262652	15.116506	-0.062978	4.442364
317.938965	6777.218082	15.121511	-0.062971	4.439765
317.557766	6769.310021	15.126515	-0.062894	4.437208
317.509582	6761.235014	15.131520	-0.062880	4.434597
317.435956	6753.265554	15.136525	-0.062861	4.432018
317.803453	6745.185147	15.141530	-0.062924	4.429404
317.612590	6737.155766	15.146535	-0.062884	4.426802
317.212292	6729.255274	15.151539	-0.062804	4.424239
317.057713	6721.293532	15.156544	-0.062770	4.421657
316.797263	6713.197996	15.161549	-0.062716	4.419028
317.326632	6705.224637	15.166554	-0.062809	4.416442
317.083188	6697.180683	15.171559	-0.062759	4.413828
317.106584	6689.171183	15.176563	-0.062758	4.411224
317.323572	6681.120534	15.181568	-0.062793	4.408607
317.072723	6673.186122	15.186573	-0.062741	4.406023
317.642161	6665.149622	15.191578	-0.062842	4.403410
317.015311	6657.230985	15.196583	-0.062720	4.400826
317.064583	6649.268554	15.201587	-0.062724	4.398230
317.452817	6641.206498	15.206592	-0.062791	4.395603
316.396868	6633.324342	15.211597	-0.062589	4.393023
316.852122	6625.276204	15.216602	-0.062668	4.390398
316.690222	6617.265365	15.221607	-0.062633	4.387778
316.636091	6609.219936	15.226611	-0.062618	4.385147
317.306749	6601.193855	15.231616	-0.062737	4.382526
317.004241	6593.190848	15.236621	-0.062676	4.379904
316.623854	6585.327797	15.241626	-0.062600	4.377325
316.328835	6577.273470	15.246631	-0.062539	4.374683
317.070274	6569.189394	15.251635	-0.062672	4.372037
316.925654	6561.249047	15.256640	-0.062640	4.369430
316.733633	6553.258470	15.261645	-0.062599	4.366805
316.733700	6545.267576	15.266650	-0.062594	4.364179
316.849053	6537.317843	15.271655	-0.062610	4.361566
316.834531	6529.280890	15.276659	-0.062602	4.358922
316.699791	6521.316985	15.281664	-0.062572	4.356300
316.643821	6513.243368	15.286669	-0.062556	4.353640
316.356715	6505.286126	15.291674	-0.062497	4.351015
316.277434	6497.225801	15.296679	-0.062477	4.348357
316.113398	6489.249053	15.301683	-0.062441	4.345723
316.214047	6481.278498	15.306688	-0.062455	4.343092
316.163028	6473.220009	15.311693	-0.062440	4.340430
315.979321	6465.286761	15.316698	-0.062401	4.337805
315.431359	6457.329503	15.321703	-0.062294	4.335169
315.992595	6449.270943	15.326707	-0.062393	4.332506
315.964340	6441.220360	15.331712	-0.062382	4.329840
315.877430	6433.244025	15.336717	-0.062361	4.327196
315.963058	6425.224046	15.341722	-0.062371	4.324537
315.689747	6417.299875	15.346727	-0.062315	4.321905
315.775262	6409.237086	15.351731	-0.062326	4.319229
315.327820	6401.362982	15.356736	-0.062237	4.316610
315.262277	6393.217331	15.361741	-0.062220	4.313901
315.380893	6385.270954	15.366746	-0.062237	4.311259
315.261063	6377.224074	15.371751	-0.062209	4.308580
314.939553	6369.275677	15.376755	-0.062144	4.305930
315.069086	6361.211663	15.381760	-0.062163	4.303244
315.051222	6353.223981	15.386765	-0.062154	4.300580
315.186248	6345.282033	15.391770	-0.062174	4.297931
315.112561	6337.217869	15.396775	-0.062155	4.295238
315.681695	6329.200979	15.401779	-0.062256	4.292565
315.654043	6321.150241	15.406784	-0.062245	4.289874
315.552718	6313.205526	15.411789	-0.062221	4.287215
315.114792	6305.232310	15.416794	-0.062135	4.284543
314.740535	6297.286690	15.421799	-0.062060	4.281878
315.256560	6289.143975	15.426803	-0.062150	4.279154
314.894832	6281.278881	15.431808	-0.062078	4.276513
314.841191	6273.243446	15.436813	-0.062063	4.273816
314.833375	6265.222011	15.441818	-0.062056	4.271123
314.780005	6257.154025	15.446823	-0.062041	4.268412
314.755467	6249.201752	15.451827	-0.062031	4.265738
314.364113	6241.260674	15.456832	-0.061953	4.263063
314.749154	6233.190409	15.461837	-0.062019	4.260350
314.913664	6225.178063	15.466842	-0.062045	4.257653
315.185925	6217.144341	15.471847	-0.062090	4.254948
314.865629	6209.223347	15.476851	-0.062025	4.252274
314.229255	6201.233877	15.481856	-0.061901	4.249571
314.532888	6193.173771	15.486861	-0.061953	4.246852
314.719189	6185.133419	15.491866	-0.061982	4.244137
314.657430	6177.216620	15.496871	-0.061965	4.241460
314.134637	6169.253773	15.501875	-0.061863	4.238760
314.222756	6161.277920	15.506880	-0.061874	4.236061
314.193350	6153.159752	15.511885	-0.061863	4.233310
314.421835	6145.177689	15.516890	-0.061900	4.230607
314.340358	6137.198615	15.521895	-0.061880	4.227900
314.216448	6129.164453	15.526899	-0.061852	4.225171
314.335464	6121.201174	15.531904	-0.061869	4.222468
314.276913	6113.176199	15.536909	-0.061852	4.219740
314.689962	6105.187773	15.541914	-0.061924	4.217028
314.300592	6097.173951	15.546919	-0.061846	4.214297
314.038867	6089.218080	15.551923	-0.061792	4.211584
313.873081	6081.232185	15.556928	-0.061756	4.208861
313.812574	6073.167446	15.561933	-0.061740	4.206111
313.894630	6065.194673	15.566938	-0.061750	4.203392
313.876758	6057.179237	15.571943	-0.061741	4.200655
313.766700	6049.229743	15.576947	-0.061715	4.197938
313.741057	6041.204033	15.581952	-0.061705	4.195194
313.996049	6033.089044	15.586957	-0.061747	4.192421
313.369180	6025.190505	15.591962	-0.061626	4.189710
313.612784	6017.125689	15.596967	-0.061666	4.186950
313.991142	6009.048614	15.601971	-0.061731	4.184186
314.031702	6001.172478	15.606976	-0.061733	4.181486
313.802796	5993.159130	15.611981	-0.061685	4.178733
313.784052	5985.198183	15.616986	-0.061677	4.175998
313.778929	5977.155700	15.621991	-0.061670	4.173234
312.934924	5969.235975	15.626995	-0.061508	4.170500
312.832283	5961.240463	15.632000	-0.061484	4.167748
312.676970	5953.174261	15.637005	-0.061449	4.164968
313.076994	5945.201825	15.642010	-0.061519	4.162226
313.115411	5937.167267	15.647015	-0.061520	4.159456
313.204487	5929.172357	15.652019	-0.061532	4.156699
313.128567	5921.192488	15.657024	-0.061512	4.153943
313.239428	5913.171209	15.662029	-0.061528	4.151173
313.676216	5905.159220	15.667034	-0.061604	4.148409
313.413816	5897.171649	15.672039	-0.061550	4.145642
313.378790	5889.184481	15.677043	-0.061538	4.142877
313.126934	5881.223573	15.682048	-0.061486	4.140116
312.402953	5873.286234	15.687053	-0.061346	4.137354
312.862158	5865.217023	15.692058	-0.061426	4.134562
313.002694	5857.175343	15.697063	-0.061447	4.131772
312.171333	5849.258730	15.702067	-0.061287	4.129011
312.419102	5841.223739	15.707072	-0.061328	4.126221
312.370861	5833.194984	15.712077	-0.061313	4.123428
312.573523	5825.225426	15.717082	-0.061346	4.120657
312.772965	5817.203035	15.722087	-0.061378	4.117866
312.672707	5809.252617	15.727091	-0.061354	4.115093
312.750600	5801.211856	15.732096	-0.061363	4.112290
312.510915	5793.186692	15.737101	-0.061313	4.109486
313.031929	5785.160382	15.742106	-0.061405	4.106690
312.884741	5777.145132	15.747111	-0.061372	4.103887
312.371686	5769.274456	15.752115	-0.061272	4.101127
312.092519	5761.256986	15.757120	-0.061214	4.098317
312.388921	5753.182130	15.762125	-0.061264	4.095494
312.309458	5745.226302	15.767130	-0.061244	4.092705
311.902799	5737.234413	15.772135	-0.061163	4.089896
311.526997	5729.266463	15.777139	-0.061088	4.087094
311.549627	5721.228703	15.782144	-0.061087	4.084272
311.612355	5713.239206	15.787149	-0.061093	4.081465
311.010238	5705.312734	15.792154	-0.060976	4.078669
311.198899	5697.234026	15.797159	-0.061006	4.075829
311.177805	5689.203552	15.802163	-0.060997	4.073001
311.200777	5681.210429	15.807168	-0.060996	4.070184
311.018846	5673.226394	15.812173	-0.060957	4.067366
310.945135	5665.214085	15.817178	-0.060938	4.064538
310.814876	5657.242562	15.822183	-0.060908	4.061721
310.911256	5649.196919	15.827187	-0.060921	4.058879
310.819356	5641.261371	15.832192	-0.060898	4.056071
311.000590	5633.149062	15.837197	-0.060927	4.053203
310.849120	5625.212325	15.842202	-0.060893	4.050390
311.146277	5617.198616	15.847207	-0.060944	4.047555
310.570912	5609.226001	15.852211	-0.060831	4.044719
310.758989	5601.261790	15.857216	-0.060861	4.041896
311.040492	5593.139776	15.862221	-0.060908	4.039016
310.808325	5585.294430	15.867226	-0.060860	4.036224
311.004785	5577.150722	15.872231	-0.060891	4.033332
311.076226	5569.171978	15.877235	-0.060899	4.030493
311.176110	5561.195771	15.882240	-0.060912	4.027654
310.284349	5553.252562	15.887245	-0.060741	4.024809
310.711968	5545.248033	15.892250	-0.060815	4.021962
311.287121	5537.135442	15.897255	-0.060917	4.019076
311.392006	5529.182390	15.902259	-0.060931	4.016237
311.217454	5521.200890	15.907264	-0.060894	4.013382
311.178306	5513.186478	15.912269	-0.060881	4.010515
311.114589	5505.230433	15.917274	-0.060864	4.007666
311.272426	5497.185892	15.922279	-0.060888	4.004788
310.983938	5489.324246	15.927283	-0.060829	4.001965
310.812469	5481.285158	15.932288	-0.060792	3.999079
310.682314	5473.321264	15.937293	-0.060763	3.996218
311.014558	5465.238268	15.942298	-0.060819	3.993321
310.623990	5457.252502	15.947303	-0.060741	3.990444
310.008813	5449.344340	15.952307	-0.060621	3.987588
310.331898	5441.258382	15.957312	-0.060676	3.984683
310.309890	5433.286965	15.962317	-0.060667	3.981811
310.495085	5425.247906	15.967322	-0.060696	3.978917
310.240316	5417.310791	15.972327	-0.060643	3.976049
310.220401	5409.250285	15.977331	-0.060634	3.973138
310.337125	5401.238126	15.982336	-0.060651	3.970246
310.367867	5393.225709	15.987341	-0.060651	3.967350
310.410630	5385.244411	15.992346	-0.060654	3.964463
310.494836	5377.315956	15.997351	-0.060665	3.961594
310.652851	5369.273200	16.002355	-0.060689	3.958682
310.099571	5361.345613	16.007360	-0.060580	3.955798
310.043147	5353.281733	16.012365	-0.060565	3.952870
309.762420	5345.305816	16.017370	-0.060507	3.949969
309.748245	5337.267222	16.022375	-0.060499	3.947047
309.419936	5329.248230	16.027379	-0.060433	3.944125
309.352063	5321.334169	16.032384	-0.060415	3.941243
309.053381	5313.330825	16.037389	-0.060354	3.938322
308.914671	5305.303798	16.042394	-0.060323	3.935394
308.954416	5297.293998	16.047399	-0.060325	3.932473
308.888957	5289.236680	16.052403	-0.060308	3.929531
308.788418	5281.344473	16.057408	-0.060284	3.926646
309.134263	5273.222766	16.062413	-0.060343	3.923683
309.289857	5265.287770	16.067418	-0.060367	3.920783
309.459993	5257.292175	16.072423	-0.060393	3.917859
309.635164	5249.265588	16.077427	-0.060420	3.914921
309.448153	5241.325700	16.082432	-0.060380	3.912006
308.913581	5233.345073	16.087437	-0.060276	3.909067
309.101636	5225.319676	16.092442	-0.060305	3.906124
309.410340	5217.255487	16.097447	-0.060357	3.903166
308.902009	5209.330071	16.102451	-0.060258	3.900241
308.815780	5201.383495	16.107456	-0.060236	3.897315
308.715439	5193.314921	16.112461	-0.060212	3.894341
308.868999	5185.362180	16.117466	-0.060236	3.891412
308.708500	5177.325289	16.122471	-0.060201	3.888444
308.950394	5169.277358	16.127475	-0.060240	3.885478
308.903610	5161.393455	16.132480	-0.060226	3.882564
308.859161	5153.351620	16.137485	-0.060213	3.879590
308.880113	5145.396653	16.142490	-0.060211	3.876647
308.333811	5137.413897	16.147495	-0.060105	3.873679
308.405314	5129.267893	16.152499	-0.060112	3.870662
308.563917	5121.273901	16.157504	-0.060137	3.867701
308.386685	5113.287401	16.162509	-0.060099	3.864732
308.344959	5105.343080	16.167514	-0.060086	3.861781
308.559471	5097.333949	16.172519	-0.060120	3.858808
308.731576	5089.292234	16.177523	-0.060147	3.855820
308.484453	5081.371363	16.182528	-0.060096	3.852865
308.606657	5073.297973	16.187533	-0.060113	3.849860
308.388588	5065.346819	16.192538	-0.060067	3.846890
308.383832	5057.311721	16.197543	-0.060061	3.843892
308.480582	5049.392291	16.202547	-0.060074	3.840936
308.019843	5041.439767	16.207552	-0.059983	3.837953
307.898316	5033.383593	16.212557	-0.059955	3.834937
308.259244	5025.376229	16.217562	-0.060017	3.831948
308.110663	5017.362622	16.222567	-0.059984	3.828942
308.238479	5009.354789	16.227571	-0.060003	3.825943
307.693163	5001.427365	16.232576	-0.059896	3.822956
307.888736	4993.402289	16.237581	-0.059927	3.819946
307.440335	4985.480176	16.242586	-0.059838	3.816959
307.589241	4977.360124	16.247591	-0.059861	3.813908
307.604583	4969.398821	16.252595	-0.059858	3.810912
307.099569	4961.476095	16.257600	-0.059759	3.807915
306.957112	4953.426906	16.262605	-0.059727	3.804877
306.961323	4945.509267	16.267610	-0.059723	3.801890
306.564841	4937.521512	16.272615	-0.059644	3.798864
306.809222	4929.429184	16.277619	-0.059684	3.795812
307.185434	4921.388791	16.282624	-0.059749	3.792779
306.706676	4913.427187	16.287629	-0.059654	3.789754
307.018617	4905.388638	16.292634	-0.059707	3.786716
306.925598	4897.398827	16.297639	-0.059685	3.783685
307.261974	4889.355015	16.302643	-0.059742	3.780641
307.142370	4881.430661	16.307648	-0.059714	3.777629
306.827980	4873.446879	16.312653	-0.059651	3.774587
306.687834	4865.500571	16.317658	-0.059619	3.771561
306.633150	4857.456127	16.322663	-0.059604	3.768497
306.769665	4849.425826	16.327667	-0.059624	3.765441
307.205903	4841.428819	16.332672	-0.059700	3.762403
306.996361	4833.429277	16.337677	-0.059656	3.759345
306.880394	4825.521075	16.342682	-0.059629	3.756322
306.434682	4817.541602	16.347687	-0.059541	3.753261
306.682293	4809.477023	16.352691	-0.059581	3.750182
306.041176	4801.592745	16.357696	-0.059457	3.747148
305.484892	4793.542700	16.362701	-0.059348	3.744050
306.005254	4785.515281	16.367706	-0.059440	3.740984
305.740997	4777.497218	16.372711	-0.059385	3.737900
305.724217	4769.499018	16.377715	-0.059377	3.734827
305.829433	4761.496194	16.382720	-0.059391	3.731754
306.006177	4753.476580	16.387725	-0.059419	3.728672
305.989798	4745.506205	16.392730	-0.059411	3.725603
305.538968	4737.596968	16.397735	-0.059321	3.722543
305.811458	4729.505019	16.402739	-0.059367	3.719429
305.708008	4721.613622	16.407744	-0.059342	3.716380
305.573449	4713.470730	16.412749	-0.059312	3.713231
305.884740	4705.430970	16.417754	-0.059365	3.710130
305.543933	4697.524483	16.422759	-0.059296	3.707061
305.686673	4689.452063	16.427763	-0.059317	3.703938
305.202030	4681.629867	16.432768	-0.059222	3.700893
305.061619	4673.542551	16.437773	-0.059190	3.697752
304.951461	4665.561392	16.442778	-0.059165	3.694650
304.320539	4657.638394	16.447783	-0.059042	3.691554
304.638115	4649.524588	16.452787	-0.059096	3.688407
304.906418	4641.521138	16.457792	-0.059140	3.685298
304.393132	4633.633895	16.462797	-0.059040	3.682211
304.899241	4625.517067	16.467802	-0.059129	3.679060
305.050256	4617.550558	16.472807	-0.059151	3.675955
305.090294	4609.554439	16.477811	-0.059154	3.672832
304.932207	4601.584411	16.482816	-0.059119	3.669712
304.937423	4593.529348	16.487821	-0.059115	3.666561
304.978044	4585.568797	16.492826	-0.059117	3.663444
304.779324	4577.613401	16.497831	-0.059075	3.660321
304.317011	4569.669022	16.502835	-0.058983	3.657191
305.152301	4561.514995	16.507840	-0.059134	3.654013
305.128621	4553.579832	16.512845	-0.059124	3.650894
305.006776	4545.621894	16.517850	-0.059096	3.647761
304.897997	4537.643767	16.522855	-0.059071	3.644617
304.871463	4529.692882	16.527859	-0.059060	3.641484
305.049601	4521.686810	16.532864	-0.059088	3.638332
304.947295	4513.685471	16.537869	-0.059064	3.635171
304.529359	4505.749273	16.542874	-0.058981	3.632025
304.281385	4497.734547	16.547879	-0.058930	3.628849
304.453689	4489.665969	16.552883	-0.058956	3.625661
304.702263	4481.655645	16.557888	-0.058997	3.622496
304.301223	4473.652747	16.562893	-0.058917	3.619312
304.561788	4465.674389	16.567898	-0.058961	3.616154
304.341411	4457.686773	16.572903	-0.058914	3.612976
304.080719	4449.720222	16.577907	-0.058861	3.609802
304.277140	4441.699934	16.582912	-0.058892	3.606617
304.495544	4433.648982	16.587917	-0.058927	3.603418
304.278955	4425.746681	16.592922	-0.058882	3.600263
303.835900	4417.801590	16.597927	-0.058794	3.597081
304.079723	4409.711380	16.602931	-0.058834	3.593858
304.069513	4401.790057	16.607936	-0.058827	3.590693
303.574808	4393.781392	16.612941	-0.058730	3.587475
303.330509	4385.756824	16.617946	-0.058679	3.584256
303.149987	4377.834520	16.622951	-0.058640	3.581076
303.167612	4369.797120	16.627955	-0.058638	3.577854
303.097511	4361.793756	16.632960	-0.058620	3.574639
302.888376	4353.812747	16.637965	-0.058576	3.571427
302.807623	4345.828562	16.642970	-0.058555	3.568214
303.177024	4337.728406	16.647975	-0.058619	3.564965
303.304197	4329.762288	16.652979	-0.058637	3.561760
303.117739	4321.866595	16.657984	-0.058597	3.558571
303.069013	4313.811372	16.662989	-0.058583	3.555319
303.009650	4305.779040	16.667994	-0.058567	3.552073
302.860690	4297.776381	16.672999	-0.058534	3.548833
302.951623	4289.744951	16.678003	-0.058545	3.545585
302.819304	4281.808136	16.683008	-0.058515	3.542367
303.018580	4273.750640	16.688013	-0.058547	3.539106
303.001841	4265.823319	16.693018	-0.058539	3.535889
302.407552	4257.898067	16.698023	-0.058423	3.532652
302.522066	4249.836215	16.703027	-0.058439	3.529378
302.425339	4241.902558	16.708032	-0.058416	3.526147
302.482384	4233.837785	16.713037	-0.058421	3.522864
302.684914	4225.831120	16.718042	-0.058454	3.519606
303.052527	4217.844823	16.723047	-0.058517	3.516359
302.964343	4209.865699	16.728051	-0.058495	3.513098
303.086626	4201.844601	16.733056	-0.058513	3.509823
302.836520	4193.900047	16.738061	-0.058461	3.506564
303.097787	4185.878265	16.743066	-0.058504	3.503287
302.921264	4177.943578	16.748071	-0.058466	3.500029
302.080512	4170.015286	16.753075	-0.058304	3.496748
302.224377	4161.988084	16.758080	-0.058326	3.493456
301.887192	4153.975017	16.763085	-0.058258	3.490151
301.966803	4145.967347	16.768090	-0.058267	3.486858
301.907845	4137.946536	16.773095	-0.058251	3.483553
302.645389	4129.860061	16.778099	-0.058383	3.480243
302.457237	4121.991879	16.783104	-0.058343	3.476990
302.034706	4114.036063	16.788109	-0.058259	3.473690
301.754761	4106.076428	16.793114	-0.058202	3.470390
301.567786	4098.073952	16.798119	-0.058162	3.467072
301.230542	4090.040267	16.803123	-0.058094	3.463732
301.504404	4082.020195	16.808128	-0.058139	3.460416
301.413757	4074.003742	16.813133	-0.058117	3.457086
301.435251	4066.021147	16.818138	-0.058116	3.453770
301.203421	4058.034814	16.823143	-0.058067	3.450441
301.195974	4050.034775	16.828147	-0.058061	3.447111
300.916006	4042.096486	16.833152	-0.058003	3.443794
300.850884	4034.092789	16.838157	-0.057986	3.440454
301.433257	4025.998211	16.843162	-0.058089	3.437095
300.723991	4018.130944	16.848167	-0.057952	3.433783
300.761344	4010.130897	16.853171	-0.057954	3.430438
300.882607	4002.109257	16.858176	-0.057971	3.427084
300.535412	3994.104205	16.863181	-0.057901	3.423716
300.988912	3986.062901	16.868186	-0.057980	3.420359
301.236365	3978.080842	16.873191	-0.058021	3.417016
301.311086	3970.070597	16.878195	-0.058030	3.413652
301.390348	3962.080441	16.883200	-0.058039	3.410293
300.939456	3954.143871	16.888205	-0.057950	3.406934
300.620652	3946.215947	16.893210	-0.057885	3.403580
300.790686	3938.189974	16.898215	-0.057912	3.400200
300.469627	3930.224962	16.903219	-0.057847	3.396824
300.111921	3922.274116	16.908224	-0.057775	3.393449
300.195722	3914.176964	16.913229	-0.057785	3.390024
300.346703	3906.145514	16.918234	-0.057808	3.386627
300.323251	3898.159909	16.923239	-0.057799	3.383239
300.235608	3890.198157	16.928243	-0.057777	3.379856
300.531563	3882.198710	16.933248	-0.057827	3.376467
299.899258	3874.251809	16.938253	-0.057704	3.373064
299.739766	3866.264031	16.943258	-0.057669	3.369656
299.818998	3858.267253	16.948263	-0.057678	3.366250
299.522347	3850.290181	16.953267	-0.057618	3.362836
299.726850	3842.273805	16.958272	-0.057651	3.359419
299.909190	3834.264517	16.963277	-0.057679	3.356001
300.016686	3826.269161	16.968282	-0.057694	3.352583
299.979566	3818.258977	16.973287	-0.057682	3.349150
299.794051	3810.310886	16.978291	-0.057642	3.345734
299.999633	3802.330553	16.983296	-0.057675	3.342316
299.428258	3794.393125	16.988301	-0.057564	3.338883
299.494670	3786.384195	16.993306	-0.057571	3.335440
299.433804	3778.391955	16.998311	-0.057554	3.331996
299.663956	3770.292983	17.003315	-0.057592	3.328513
300.170036	3762.281800	17.008320	-0.057681	3.325076
300.040567	3754.346521	17.013325	-0.057651	3.321643
299.704396	3746.395525	17.018330	-0.057584	3.318192
299.414827	3738.453092	17.023335	-0.057524	3.314742
299.095213	3730.487219	17.028339	-0.057460	3.311278
298.859941	3722.503508	17.033344	-0.057411	3.307805
298.449157	3714.470206	17.038349	-0.057329	3.304300
299.250610	3706.402925	17.043354	-0.057473	3.300825
299.180607	3698.438905	17.048359	-0.057455	3.297356
299.197588	3690.435968	17.053363	-0.057452	3.293870
298.981626	3682.474252	17.058368	-0.057407	3.290390
299.056295	3674.478707	17.063373	-0.057416	3.286902
299.036490	3666.506718	17.068378	-0.057407	3.283417
298.661203	3658.563802	17.073383	-0.057332	3.279927
298.755392	3650.552736	17.078387	-0.057344	3.276423
298.874832	3642.542885	17.083392	-0.057361	3.272916
298.513041	3634.561254	17.088397	-0.057288	3.269398
298.103913	3626.668776	17.093402	-0.057207	3.265913
297.754847	3618.674346	17.098407	-0.057137	3.262383
297.782296	3610.629558	17.103411	-0.057136	3.258841
298.080114	3602.591611	17.108416	-0.057187	3.255310
297.673984	3594.650755	17.113421	-0.057106	3.251789
297.810201	3586.638172	17.118426	-0.057126	3.248255
297.762257	3578.614160	17.123431	-0.057112	3.244705
298.183390	3570.591432	17.128435	-0.057185	3.241170
297.885703	3562.700701	17.133440	-0.057124	3.237660
297.715496	3554.660347	17.138445	-0.057087	3.234086
297.876094	3546.680517	17.143450	-0.057112	3.230548
297.534044	3538.732516	17.148455	-0.057043	3.226999
297.779842	3530.639376	17.153459	-0.057083	3.223407
297.920569	3522.663176	17.158464	-0.057104	3.219858
297.743202	3514.670140	17.163469	-0.057066	3.216284
298.077575	3506.644782	17.168474	-0.057123	3.212714
297.798720	3498.695371	17.173479	-0.057066	3.209147
297.394586	3490.790677	17.178483	-0.056985	3.205591
297.837180	3482.759113	17.183488	-0.057063	3.202011
297.726454	3474.738242	17.188493	-0.057037	3.198407
297.450431	3466.848040	17.193498	-0.056980	3.194851
297.603272	3458.816274	17.198503	-0.057003	3.191246
297.516875	3450.798018	17.203507	-0.056982	3.187633
297.642968	3442.781388	17.208512	-0.057000	3.184026
297.781800	3434.792597	17.213517	-0.057021	3.180427
297.499982	3426.873889	17.218522	-0.056963	3.176838
297.301332	3418.920948	17.223527	-0.056921	3.173233
297.099197	3410.900988	17.228531	-0.056878	3.169593
297.339581	3402.895066	17.233536	-0.056917	3.165975
297.581289	3394.855416	17.238541	-0.056957	3.162337
297.078301	3386.960150	17.243546	-0.056858	3.158728
297.370677	3378.950296	17.248551	-0.056908	3.155098
297.342383	3370.933297	17.253555	-0.056897	3.151446
297.471056	3362.927833	17.258560	-0.056916	3.147802
296.914904	3354.997588	17.263565	-0.056807	3.144158
297.101449	3347.006959	17.268570	-0.056836	3.140515
297.424292	3338.952574	17.273575	-0.056891	3.136845
297.265828	3330.978050	17.278579	-0.056856	3.133185
297.327174	3322.971858	17.283584	-0.056863	3.129517
296.767321	3315.080860	17.288589	-0.056753	3.125869
296.831977	3307.072077	17.293594	-0.056760	3.122191
296.956003	3299.076891	17.298599	-0.056778	3.118517
296.617344	3291.155373	17.303603	-0.056710	3.114852
296.625776	3283.162255	17.308608	-0.056706	3.111166
296.041029	3275.220465	17.313613	-0.056592	3.107471
296.634095	3267.079781	17.318618	-0.056697	3.103735
296.237965	3259.193447	17.323623	-0.056618	3.100065
295.942168	3251.241800	17.328627	-0.056558	3.096366
295.928599	3243.231995	17.333632	-0.056550	3.092649
296.222654	3235.154024	17.338637	-0.056599	3.088910
296.750643	3227.095923	17.343642	-0.056692	3.085187
296.891394	3219.142650	17.348647	-0.056713	3.081490
296.453982	3211.239585	17.353651	-0.056627	3.077784
296.533141	3203.248917	17.358656	-0.056636	3.074057
295.940199	3195.283220	17.363661	-0.056520	3.070306
296.177052	3187.253065	17.368666	-0.056559	3.066559
296.078351	3179.284693	17.373671	-0.056536	3.062821
296.111609	3171.264514	17.378675	-0.056537	3.059060
296.133140	3163.331131	17.383680	-0.056535	3.055335
296.066108	3155.334373	17.388685	-0.056518	3.051571
296.063058	3147.328247	17.393690	-0.056512	3.047801
295.704483	3139.385764	17.398695	-0.056440	3.044039
296.089352	3131.364802	17.403699	-0.056506	3.040272
296.039795	3123.434844	17.408704	-0.056492	3.036522
295.421625	3115.498688	17.413709	-0.056371	3.032736
295.563632	3107.441297	17.418714	-0.056393	3.028926
295.891349	3099.401334	17.423719	-0.056448	3.025128
295.594879	3091.462273	17.428723	-0.056388	3.021342
295.666863	3083.508058	17.433728	-0.056396	3.017563
295.514121	3075.522756	17.438733	-0.056362	3.013753
295.569205	3067.501976	17.443738	-0.056367	3.009932
295.556251	3059.541085	17.448743	-0.056360	3.006131
295.362522	3051.589328	17.453747	-0.056318	3.002320
295.576848	3043.588497	17.458752	-0.056353	2.998502
295.739735	3035.568097	17.463757	-0.056378	2.994667
296.067268	3027.558428	17.468762	-0.056434	2.990840
295.727117	3019.629312	17.473767	-0.056365	2.987013
295.595144	3011.616127	17.478771	-0.056336	2.983152
295.405078	3003.718112	17.483776	-0.056295	2.979338
295.382918	2995.722892	17.488781	-0.056286	2.975481
294.733597	2987.802077	17.493786	-0.056159	2.971621
294.623895	2979.803043	17.498791	-0.056134	2.967748
294.564875	2971.777431	17.503795	-0.056118	2.963859
294.580353	2963.829568	17.508800	-0.056115	2.960006
294.589780	2955.829080	17.513805	-0.056112	2.956123
294.116166	2947.887373	17.518810	-0.056018	2.952237
294.373346	2939.858458	17.523815	-0.056061	2.948342
294.027937	2931.867024	17.528819	-0.055991	2.944429
294.527982	2923.843419	17.533824	-0.056079	2.940540
294.554642	2915.866918	17.538829	-0.056079	2.936643
294.752759	2907.871257	17.543834	-0.056110	2.932742
294.217934	2899.947941	17.548839	-0.056006	2.928830
294.415522	2891.901088	17.553843	-0.056037	2.924893
294.149048	2884.007181	17.558848	-0.055982	2.921000
293.218308	2876.167848	17.563853	-0.055804	2.917092
293.664914	2868.023012	17.568858	-0.055882	2.913104
293.300110	2860.049014	17.573863	-0.055809	2.909151
293.601694	2851.968138	17.578867	-0.055859	2.905176
293.687354	2844.013741	17.583872	-0.055870	2.901246
294.033914	2835.964659	17.588877	-0.055929	2.897278
293.929600	2828.043019	17.593882	-0.055905	2.893343
293.955149	2820.017123	17.598887	-0.055904	2.889358
294.049426	2812.040971	17.603891	-0.055917	2.885396
294.022512	2804.153902	17.608896	-0.055906	2.881466
293.768039	2796.191950	17.613901	-0.055854	2.877481
293.247976	2788.264956	17.618906	-0.055752	2.873493
293.001224	2780.290217	17.623911	-0.055701	2.869490
293.395339	2772.194834	17.628915	-0.055769	2.865458
293.945755	2764.158800	17.633920	-0.055866	2.861459
293.598987	2756.271268	17.638925	-0.055796	2.857478
293.547528	2748.301062	17.643930	-0.055781	2.853467
293.298530	2740.346698	17.648935	-0.055730	2.849446
293.545360	2732.303033	17.653939	-0.055770	2.845404
293.507998	2724.399602	17.658944	-0.055758	2.841410
293.149416	2716.444265	17.663949	-0.055686	2.837365
292.744794	2708.521777	17.668954	-0.055606	2.833329
293.305819	2700.403596	17.673959	-0.055705	2.829243
293.171917	2692.424935	17.678963	-0.055675	2.825183
292.749937	2684.536503	17.683968	-0.055591	2.821145
292.711578	2676.536177	17.688973	-0.055578	2.817067
292.815815	2668.513794	17.693978	-0.055593	2.812980
292.285052	2660.634794	17.698983	-0.055489	2.808923
292.406966	2652.576887	17.703987	-0.055506	2.804807
292.525256	2644.626138	17.708992	-0.055523	2.800740
291.984252	2636.724334	17.713997	-0.055417	2.796653
291.890647	2628.744421	17.719002	-0.055394	2.792546
291.876265	2620.712463	17.724007	-0.055386	2.788412
292.013716	2612.669163	17.729011	-0.055406	2.784274
291.613637	2604.810909	17.734016	-0.055327	2.780193
291.684644	2596.768954	17.739021	-0.055335	2.776040
291.745662	2588.766683	17.744026	-0.055341	2.771901
291.823815	2580.771297	17.749031	-0.055350	2.767760
291.409370	2572.840703	17.754035	-0.055268	2.763616
291.929155	2564.806132	17.759040	-0.055359	2.759469
291.324726	2556.941334	17.764045	-0.055242	2.755335
291.500455	2548.852402	17.769050	-0.055269	2.751127
291.617001	2540.861015	17.774055	-0.055285	2.746959
291.730775	2532.853402	17.779059	-0.055301	2.742776
291.651760	2524.941691	17.784064	-0.055281	2.738625
291.761750	2516.937375	17.789069	-0.055297	2.734431
292.147729	2508.935938	17.794074	-0.055363	2.730249
291.791517	2501.036816	17.799079	-0.055292	2.726068
291.529195	2493.079558	17.804083	-0.055238	2.721856
291.806592	2485.097534	17.809088	-0.055284	2.717658
291.917897	2477.091683	17.814093	-0.055300	2.713431
290.817959	2469.277549	17.819098	-0.055090	2.709221
291.253639	2461.192770	17.824103	-0.055165	2.704960
291.184540	2453.225097	17.829107	-0.055147	2.700721
291.191171	2445.267224	17.834112	-0.055143	2.696486
291.213620	2437.221609	17.839117	-0.055142	2.692199
291.045428	2429.286797	17.844122	-0.055106	2.687952
290.726473	2421.387093	17.849127	-0.055041	2.683706
290.503815	2413.407351	17.854131	-0.054994	2.679418
291.126667	2405.379508	17.859136	-0.055105	2.675152
290.881824	2397.428058	17.864141	-0.055054	2.670863
291.018281	2389.399248	17.869146	-0.055074	2.666551
290.960147	2381.442563	17.874151	-0.055058	2.662258
290.618796	2373.511660	17.879155	-0.054990	2.657953
290.637424	2365.547103	17.884160	-0.054988	2.653647
290.364720	2357.569537	17.889165	-0.054932	2.649307
289.924259	2349.676544	17.894170	-0.054845	2.644995
289.790853	2341.713579	17.899175	-0.054814	2.640658
290.030655	2333.657005	17.904179	-0.054854	2.636288
290.482816	2325.624149	17.909184	-0.054933	2.631939
290.532800	2317.638085	17.914189	-0.054937	2.627580
290.204419	2309.751750	17.919194	-0.054870	2.623243
289.784623	2301.860461	17.924199	-0.054787	2.618890
290.116113	2293.790560	17.929203	-0.054844	2.614483
289.916956	2285.847895	17.934208	-0.054801	2.610102
289.854913	2277.862685	17.939213	-0.054784	2.605700
289.924970	2269.919921	17.944218	-0.054792	2.601323
289.545434	2262.030680	17.949223	-0.054716	2.596936
289.457636	2253.963832	17.954227	-0.054695	2.592464
289.266854	2245.941105	17.959232	-0.054654	2.588002
289.328556	2237.938032	17.964237	-0.054660	2.583561
289.693290	2229.920968	17.969242	-0.054723	2.579125
289.585034	2222.010458	17.974247	-0.054698	2.574708
289.755989	2214.013045	17.979251	-0.054724	2.570255
289.798513	2206.062448	17.984256	-0.054727	2.565811
289.503206	2198.165282	17.989261	-0.054667	2.561365
289.314850	2190.228068	17.994266	-0.054626	2.556897
289.588610	2182.215013	17.999271	-0.054672	2.552411
289.725055	2174.197168	18.004275	-0.054692	2.547904
289.896658	2166.224294	18.009280	-0.054719	2.543418
289.592174	2158.329230	18.014285	-0.054657	2.538933
289.181723	2150.410135	18.019290	-0.054575	2.534419
289.557450	2142.388809	18.024295	-0.054640	2.529896
289.142218	2134.458574	18.029299	-0.054558	2.525359
288.869034	2126.595454	18.034304	-0.054501	2.520863
289.054749	2118.542811	18.039309	-0.054531	2.516284
289.232798	2110.539544	18.044314	-0.054559	2.511724
289.140039	2102.610059	18.049319	-0.054536	2.507178
289.171777	2094.582291	18.054323	-0.054537	2.502577
289.152837	2086.662719	18.059328	-0.054528	2.498026
288.448643	2078.820557	18.064333	-0.054392	2.493459
288.394115	2070.798910	18.069338	-0.054376	2.488830
288.585411	2062.768470	18.074343	-0.054407	2.484205
288.043964	2054.918243	18.079347	-0.054301	2.479620
287.903894	2046.972719	18.084352	-0.054269	2.475003
288.236482	2038.896060	18.089357	-0.054326	2.470336
287.914940	2030.972117	18.094362	-0.054261	2.465699
288.039785	2022.982331	18.099367	-0.054279	2.461050
288.130653	2014.984542	18.104371	-0.054291	2.456384
287.914808	2007.086857	18.109376	-0.054245	2.451744
287.645953	1999.162064	18.114381	-0.054190	2.447076
287.631190	1991.194239	18.119386	-0.054182	2.442393
287.860359	1983.196381	18.124391	-0.054219	2.437702
288.297717	1975.111302	18.129395	-0.054296	2.432967
287.705465	1967.278037	18.134400	-0.054180	2.428291
287.765295	1959.255691	18.139405	-0.054186	2.423546
288.138662	1951.242426	18.144410	-0.054250	2.418821
288.157936	1943.295259	18.149415	-0.054249	2.414098
287.333941	1935.474551	18.154419	-0.054090	2.409374
287.006754	1927.554053	18.159424	-0.054024	2.404621
286.938317	1919.591510	18.164429	-0.054006	2.399854
287.180563	1911.570309	18.169434	-0.054046	2.395067
287.179942	1903.588807	18.174439	-0.054040	2.390275
287.511609	1895.550813	18.179443	-0.054097	2.385466
287.488846	1887.667663	18.184448	-0.054087	2.380712
287.493732	1879.699714	18.189453	-0.054083	2.375900
287.501975	1871.745638	18.194458	-0.054079	2.371086
287.410086	1863.822032	18.199463	-0.054057	2.366273
287.421400	1855.828751	18.204467	-0.054054	2.361416
287.095678	1847.946075	18.209472	-0.053988	2.356589
287.392937	1839.910939	18.214477	-0.054038	2.351710
286.850019	1832.054148	18.219482	-0.053932	2.346861
287.082981	1824.027947	18.224487	-0.053970	2.341962
286.453060	1816.171035	18.229491	-0.053848	2.337085
286.773262	1808.167512	18.234496	-0.053902	2.332187
286.540664	1800.205726	18.239501	-0.053853	2.327258
286.714045	1792.218887	18.244506	-0.053880	2.322337
286.211955	1784.396534	18.249511	-0.053782	2.317450
286.344102	1776.371586	18.254515	-0.053801	2.312481
286.242232	1768.417585	18.259520	-0.053777	2.307526
286.899598	1760.326952	18.264525	-0.053894	2.302540
286.706218	1752.447800	18.269530	-0.053853	2.297602
286.764043	1744.489423	18.274535	-0.053858	2.292626
286.786850	1736.513352	18.279539	-0.053857	2.287624
286.974467	1728.568543	18.284544	-0.053887	2.282646
286.649405	1720.714366	18.289549	-0.053821	2.277669
286.525486	1712.742908	18.294554	-0.053793	2.272624
286.119597	1704.823077	18.299559	-0.053712	2.267577
286.362924	1696.799617	18.304563	-0.053752	2.262509
286.517782	1688.835495	18.309568	-0.053776	2.257460
286.269869	1680.922889	18.314573	-0.053725	2.252397
286.494985	1672.930479	18.319578	-0.053761	2.247314
286.208427	1665.063560	18.324583	-0.053703	2.242253
286.074785	1657.123102	18.329587	-0.053673	2.237148
285.626119	1649.261645	18.334592	-0.053584	2.232053
285.834233	1641.231577	18.339597	-0.053617	2.226897
285.773195	1633.280832	18.344602	-0.053601	2.221756
285.702626	1625.358775	18.349607	-0.053582	2.216621
285.554269	1617.408200	18.354611	-0.053550	2.211449
285.805228	1609.397720	18.359616	-0.053591	2.206262
285.722020	1601.471201	18.364621	-0.053570	2.201086
285.532007	1593.595711	18.369626	-0.053530	2.195922
285.672050	1585.612677	18.374631	-0.053551	2.190706
285.671025	1577.626828	18.379635	-0.053545	2.185463
285.591089	1569.731311	18.384640	-0.053525	2.180258
285.848716	1561.716696	18.389645	-0.053568	2.174995
285.563969	1553.841474	18.394650	-0.053510	2.169760
285.398914	1545.923632	18.399655	-0.053474	2.164495
285.392531	1537.986697	18.404659	-0.053467	2.159220
285.171460	1530.107211	18.409664	-0.053421	2.153949
285.070027	1522.141015	18.414669	-0.053397	2.148620
285.011489	1514.194757	18.419674	-0.053381	2.143294
285.269326	1506.217343	18.424679	-0.053423	2.137965
284.485353	1498.406914	18.429683	-0.053272	2.132633
284.595040	1490.429223	18.434688	-0.053288	2.127263
284.906411	1482.426260	18.439693	-0.053340	2.121881
284.113665	1474.637093	18.444698	-0.053188	2.116523
284.058892	1466.655671	18.449703	-0.053172	2.111092
284.019377	1458.655987	18.454707	-0.053159	2.105637
283.990129	1450.732367	18.459712	-0.053149	2.100220
283.891765	1442.787363	18.464717	-0.053125	2.094768
284.440259	1434.746524	18.469722	-0.053222	2.089301
284.388238	1426.847030	18.474727	-0.053207	2.083856
284.074361	1418.956128	18.479731	-0.053144	2.078377
283.826813	1411.088930	18.484736	-0.053092	2.072906
283.448911	1403.196863	18.489741	-0.053017	2.067390
283.921702	1395.138316	18.494746	-0.053100	2.061830
283.338633	1387.345658	18.499751	-0.052986	2.056333
283.428426	1379.363398	18.504755	-0.052997	2.050757
283.815810	1371.342012	18.509760	-0.053064	2.045169
283.684741	1363.452175	18.514765	-0.053035	2.039605
283.988272	1355.488801	18.519770	-0.053086	2.034019
283.666801	1347.634205	18.524775	-0.053021	2.028430
283.436569	1339.715231	18.529779	-0.052973	2.022789
283.643728	1331.770728	18.534784	-0.053006	2.017159
283.625076	1323.828421	18.539789	-0.052997	2.011492
283.979127	1315.824737	18.544794	-0.053058	2.005805
283.812220	1307.964683	18.549799	-0.053022	2.000149
283.557831	1300.091039	18.554803	-0.052969	1.994457
283.381931	1292.202620	18.559808	-0.052931	1.988747
282.804505	1284.362512	18.564813	-0.052819	1.983012
282.760537	1276.437553	18.569818	-0.052805	1.977257
282.721282	1268.498559	18.574823	-0.052793	1.971475
282.420825	1260.598128	18.579827	-0.052732	1.965675
282.441109	1252.669427	18.584832	-0.052730	1.959873
282.380667	1244.765687	18.589837	-0.052714	1.954063
282.578865	1236.784080	18.594842	-0.052745	1.948207
282.752191	1228.813144	18.599847	-0.052772	1.942339
282.646674	1220.913272	18.604851	-0.052748	1.936474
282.601806	1213.021088	18.609856	-0.052734	1.930604
282.654208	1205.055176	18.614861	-0.052739	1.924672
282.239032	1197.243605	18.619866	-0.052656	1.918785
282.738398	1189.227143	18.624871	-0.052744	1.912829
282.789092	1181.285132	18.629875	-0.052748	1.906860
282.954233	1173.384368	18.634880	-0.052774	1.900916
282.084183	1165.638243	18.639885	-0.052607	1.894951
282.292838	1157.670407	18.644890	-0.052640	1.888924
282.178831	1149.778695	18.649895	-0.052614	1.882898
282.089966	1141.881755	18.654899	-0.052592	1.876851
281.861428	1134.032703	18.659904	-0.052544	1.870805
281.969481	1126.050025	18.664909	-0.052559	1.864677
282.481410	1118.059535	18.669914	-0.052649	1.858570
281.805906	1110.291573	18.674919	-0.052518	1.852474
281.857431	1102.336589	18.679923	-0.052523	1.846299
281.649385	1094.508487	18.684928	-0.052479	1.840171
281.344274	1086.650649	18.689933	-0.052417	1.833988
281.335632	1078.722531	18.694938	-0.052410	1.827765
281.671259	1070.743216	18.699943	-0.052467	1.821522
281.901099	1062.800777	18.704947	-0.052505	1.815274
281.792980	1054.955896	18.709952	-0.052480	1.809040
281.457511	1047.103674	18.714957	-0.052412	1.802750
281.556301	1039.200322	18.719962	-0.052425	1.796452
281.522323	1031.302813	18.724967	-0.052414	1.790119
281.471326	1023.387829	18.729971	-0.052399	1.783748
281.016859	1015.589342	18.734976	-0.052309	1.777397
281.035981	1007.678205	18.739981	-0.052308	1.770992
281.061683	999.766031	18.744986	-0.052307	1.764564
280.923826	991.921777	18.749991	-0.052276	1.758147
280.756331	984.049997	18.754995	-0.052240	1.751679
281.270192	976.061054	18.760000	-0.052330	1.745180
281.109762	968.214244	18.765005	-0.052295	1.738686
281.138234	960.326119	18.770010	-0.052295	1.732158
281.103096	952.468482	18.775015	-0.052284	1.725622
281.116782	944.590878	18.780019	-0.052281	1.719052
281.064012	936.748234	18.785024	-0.052266	1.712476
281.059319	928.852134	18.790029	-0.052260	1.705837
280.791010	921.033421	18.795034	-0.052205	1.699202
280.478909	913.218933	18.800039	-0.052142	1.692538
280.522937	905.287787	18.805043	-0.052145	1.685797
280.410456	897.468927	18.810048	-0.052119	1.679103
280.333625	889.599513	18.815053	-0.052099	1.672344
280.421634	881.677611	18.820058	-0.052110	1.665535
280.198828	873.874966	18.825063	-0.052064	1.658758
280.032739	866.020494	18.830067	-0.052028	1.651917
279.759744	858.200558	18.835072	-0.051972	1.645062
279.463536	850.411277	18.840077	-0.051911	1.638201
279.439096	842.505913	18.845082	-0.051902	1.631248
279.801306	834.536577	18.850087	-0.051964	1.624264
279.450223	826.744020	18.855091	-0.051893	1.617305
279.877390	818.801286	18.860096	-0.051968	1.610293
279.981125	810.929851	18.865101	-0.051982	1.603268
279.447860	803.196732	18.870106	-0.051877	1.596244
279.470817	795.342678	18.875111	-0.051877	1.589160
279.827709	787.418066	18.880115	-0.051938	1.582030
279.758214	779.600714	18.885120	-0.051920	1.574903
279.789450	771.754081	18.890125	-0.051920	1.567731
279.245260	764.028679	18.895130	-0.051814	1.560552
278.736096	756.303808	18.900135	-0.051714	1.553346
278.742855	748.399487	18.905139	-0.051710	1.546017
279.187404	740.490446	18.910144	-0.051788	1.538714
278.769439	732.734809	18.915149	-0.051705	1.531390
278.729628	724.894782	18.920154	-0.051692	1.524009
278.708462	717.087013	18.925159	-0.051683	1.516625
278.843372	709.223182	18.930163	-0.051703	1.509176
278.565685	701.464097	18.935168	-0.051646	1.501725
278.701186	693.596242	18.940173	-0.051666	1.494198
278.341055	685.843852	18.945178	-0.051594	1.486666
278.699293	677.983788	18.950183	-0.051656	1.479105
278.501610	670.181352	18.955187	-0.051614	1.471473
278.305015	662.389942	18.960192	-0.051572	1.463812
278.678153	654.509255	18.965197	-0.051636	1.456115
278.106170	646.820451	18.970202	-0.051525	1.448412
277.952254	639.058608	18.975207	-0.051491	1.440665
278.126097	631.216426	18.980211	-0.051518	1.432849
278.359113	623.377186	18.985216	-0.051557	1.425003
278.185134	615.636101	18.990221	-0.051519	1.417145
278.354239	607.823157	18.995226	-0.051545	1.409228
278.046171	600.113805	19.000231	-0.051483	1.401292
277.945958	592.345312	19.005235	-0.051459	1.393284
277.768117	584.600092	19.010240	-0.051421	1.385241
277.632765	576.855936	19.015245	-0.051391	1.377159
277.662594	569.059409	19.020250	-0.051391	1.369004
277.381927	561.350794	19.025255	-0.051334	1.360838
277.249619	553.605281	19.030259	-0.051304	1.352609
277.678395	545.764441	19.035264	-0.051379	1.344329
277.661291	538.023495	19.040269	-0.051371	1.336024
277.055291	530.397719	19.045274	-0.051253	1.327686
277.235874	522.621383	19.050279	-0.051281	1.319274
277.200599	514.832406	19.055283	-0.051269	1.310754
277.237431	507.048655	19.060288	-0.051271	1.302198
277.260635	499.325999	19.065293	-0.051270	1.293651
276.626917	491.707860	19.070298	-0.051147	1.285040
277.259221	483.883693	19.075303	-0.051260	1.276379
277.053299	476.219756	19.080307	-0.051217	1.267680
276.839307	468.555976	19.085312	-0.051172	1.258920
277.077335	460.811419	19.090317	-0.051211	1.250094
276.880345	453.155452	19.095322	-0.051169	1.241221
277.131552	445.455773	19.100327	-0.051211	1.232323
276.914954	437.787885	19.105331	-0.051166	1.223304
277.090725	430.098794	19.110336	-0.051193	1.214272
276.961088	422.450940	19.115341	-0.051164	1.205159
276.879014	414.806828	19.120346	-0.051144	1.195991
276.628893	407.210989	19.125351	-0.051092	1.186776
276.377347	399.595350	19.130355	-0.051040	1.177464
276.020925	392.018498	19.135360	-0.050969	1.168104
276.085634	384.354005	19.140365	-0.050976	1.158648
275.921576	376.735064	19.145370	-0.050941	1.149123
275.522957	369.170803	19.150375	-0.050861	1.139536
275.627976	361.508728	19.155379	-0.050876	1.129853
275.562067	353.916976	19.160384	-0.050859	1.120139
275.553343	346.319200	19.165389	-0.050852	1.110345
275.773307	338.683390	19.170394	-0.050888	1.100466
275.492930	331.168976	19.175399	-0.050831	1.090543
275.628946	323.573112	19.180403	-0.050851	1.080517
275.300919	316.087260	19.185408	-0.050785	1.070436
275.667583	308.454428	19.190413	-0.050848	1.060224
275.315223	300.989572	19.195418	-0.050778	1.049971
275.115813	293.508341	19.200423	-0.050736	1.039632
275.118225	285.985162	19.205427	-0.050731	1.029178
274.570135	278.588208	19.210432	-0.050624	1.018661
274.356468	271.123319	19.215437	-0.050580	1.008019
273.979582	263.704472	19.220442	-0.050505	0.997290
274.757737	256.051285	19.225447	-0.050644	0.986395
274.430283	248.663581	19.230451	-0.050579	0.975486
274.345589	241.244067	19.235456	-0.050558	0.964469
274.103681	233.868909	19.240461	-0.050508	0.953350
273.747591	226.519059	19.245466	-0.050437	0.942108
274.404018	219.003547	19.250471	-0.050554	0.930748
273.977787	211.715808	19.255475	-0.050470	0.919308
273.858043	204.385329	19.260480	-0.050443	0.907740
273.776288	197.061759	19.265485	-0.050423	0.896045
273.913796	189.713134	19.270490	-0.050444	0.884217
273.606458	182.484051	19.275495	-0.050382	0.872297
273.462494	175.231807	19.280499	-0.050350	0.860220
273.325770	168.007136	19.285504	-0.050320	0.848021
273.217435	160.800132	19.290509	-0.050295	0.835682
273.527574	153.516210	19.295514	-0.050348	0.823154
273.367230	146.378261	19.300519	-0.050313	0.810543
273.234432	139.251739	19.305523	-0.050284	0.797762
273.208674	132.142070	19.310528	-0.050275	0.784838
273.223505	125.045269	19.315533	-0.050273	0.771735
272.940883	118.044965	19.320538	-0.050215	0.758489
272.888248	111.032189	19.325543	-0.050201	0.745062
272.400724	104.122888	19.330547	-0.050106	0.731439
272.230135	97.202329	19.335552	-0.050069	0.717648
271.864347	90.347881	19.340557	-0.049997	0.703651
271.689044	83.494133	19.345562	-0.049960	0.689442
271.841753	76.810174	19.350567	-0.049984	0.675419