Mon Apr 19 09:15:04 2021

Number of Points = 3630
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
4.159895	0.136595	0.000000	0.000065	0.309267

4.098172	0.150864	0.005005	0.000077	0.309282
4.350878	0.098862	0.010010	0.000030	0.309253
4.589374	0.055649	0.015014	-0.000014	0.309253
4.607650	0.054423	0.020019	-0.000018	0.309263
4.362316	0.096905	0.025024	0.000028	0.309253
4.643513	0.046726	0.030029	-0.000024	0.309257
4.148550	0.139422	0.035034	0.000068	0.309270
4.422639	0.087906	0.040038	0.000017	0.309261
4.326964	0.105687	0.045043	0.000035	0.309263
4.170501	0.084619	0.050048	0.000064	0.309031
4.186090	0.061433	0.055053	0.000061	0.308936
4.015868	0.092308	0.060058	0.000093	0.308935
4.182794	0.063051	0.065062	0.000062	0.308940
4.015416	0.095251	0.070067	0.000093	0.308948
3.988343	0.097667	0.075072	0.000098	0.308937
3.939885	0.107723	0.080077	0.000107	0.308942
3.704084	0.151313	0.085082	0.000151	0.308946
3.605077	0.170466	0.090086	0.000169	0.308951
3.983958	0.098799	0.095091	0.000099	0.308937
4.129899	0.069306	0.100096	0.000072	0.308923
3.737371	0.083492	0.105101	0.000145	0.308655
3.267476	0.165843	0.110106	0.000232	0.308641
3.952904	0.037970	0.115110	0.000105	0.308625
3.683630	0.090160	0.120115	0.000155	0.308640
3.503032	0.121409	0.125120	0.000189	0.308633
3.341449	0.156068	0.130125	0.000219	0.308657
3.929088	0.044006	0.135130	0.000109	0.308632
3.576461	0.046593	0.140134	0.000175	0.308344
3.242425	0.106218	0.145139	0.000237	0.308339
3.059198	0.140388	0.150144	0.000272	0.308343
3.376482	0.081186	0.155149	0.000213	0.308335
3.440277	0.067039	0.160154	0.000201	0.308323
3.304673	0.081876	0.165158	0.000226	0.308277
3.585836	-0.020440	0.170163	0.000174	0.308036
3.715011	-0.048100	0.175168	0.000150	0.308016
4.117674	-0.121909	0.180173	0.000075	0.308013
3.920011	-0.093461	0.185178	0.000112	0.307978
3.997859	-0.172389	0.190182	0.000097	0.307673
4.506140	-0.268358	0.195187	0.000003	0.307656
4.351431	-0.240413	0.200192	0.000032	0.307655
4.234672	-0.270910	0.205197	0.000053	0.307411
4.243821	-0.286031	0.210202	0.000052	0.307348
4.215023	-0.278985	0.215206	0.000057	0.307356
4.306295	-0.353472	0.220211	0.000040	0.307083
4.412703	-0.388789	0.225216	0.000020	0.307008
4.226127	-0.352186	0.230221	0.000055	0.307020
3.679908	-0.308709	0.235226	0.000157	0.306757
3.939450	-0.356491	0.240230	0.000109	0.306754
4.292665	-0.437876	0.245235	0.000043	0.306673
4.141229	-0.467481	0.250240	0.000071	0.306403
4.114872	-0.460033	0.255245	0.000076	0.306415
3.685896	-0.423705	0.260250	0.000156	0.306219
3.789159	-0.464102	0.265254	0.000137	0.306116
3.926757	-0.495628	0.270259	0.000111	0.306085
3.362668	-0.453259	0.275264	0.000216	0.305801
3.651800	-0.506062	0.280269	0.000163	0.305799
3.672207	-0.541581	0.285274	0.000159	0.305648
4.460095	-0.714049	0.290278	0.000012	0.305510
4.136479	-0.678617	0.295283	0.000073	0.305399
3.909616	-0.683256	0.300288	0.000115	0.305181
4.205089	-0.751455	0.305293	0.000060	0.305112
4.155689	-0.795925	0.310298	0.000069	0.304858
3.860078	-0.750832	0.315302	0.000124	0.304817
4.018268	-0.836853	0.320307	0.000095	0.304545
4.241867	-0.890496	0.325312	0.000053	0.304483
3.663673	-0.830003	0.330317	0.000161	0.304271
3.671927	-0.842176	0.335322	0.000160	0.304220
3.560612	-0.882559	0.340326	0.000180	0.303931
3.562892	-0.890697	0.345331	0.000180	0.303895
3.754284	-0.986464	0.350336	0.000144	0.303604
3.978944	-1.041967	0.355341	0.000103	0.303534
3.918309	-1.085709	0.360346	0.000114	0.303272
4.002729	-1.126220	0.365350	0.000098	0.303152
3.907200	-1.140555	0.370355	0.000116	0.303001
3.731407	-1.157211	0.375360	0.000149	0.302768
3.754136	-1.182658	0.380365	0.000145	0.302666
3.989219	-1.289475	0.385370	0.000101	0.302359
4.069485	-1.327378	0.390374	0.000086	0.302248
3.593148	-1.285182	0.395379	0.000175	0.302035
4.016210	-1.404746	0.400384	0.000096	0.301830
3.974541	-1.420243	0.405389	0.000104	0.301719
3.648902	-1.427839	0.410394	0.000165	0.301399
3.598864	-1.443679	0.415398	0.000174	0.301279
3.883644	-1.535129	0.420403	0.000121	0.301088
3.613167	-1.541470	0.425408	0.000172	0.300821
3.871461	-1.612436	0.430413	0.000124	0.300705
3.992443	-1.672223	0.435418	0.000101	0.300523
3.756592	-1.683850	0.440422	0.000145	0.300261
4.063201	-1.776956	0.445427	0.000088	0.300080
3.464957	-1.708331	0.450432	0.000200	0.299887
3.797801	-1.828817	0.455437	0.000138	0.299597
4.079416	-1.921689	0.460442	0.000085	0.299395
3.310875	-1.809955	0.465446	0.000228	0.299260
3.762926	-1.961459	0.470451	0.000144	0.298924
3.676521	-1.989155	0.475456	0.000161	0.298714
3.599570	-2.012080	0.480461	0.000175	0.298535
3.900064	-2.118889	0.485466	0.000119	0.298282
3.883190	-2.171282	0.490470	0.000122	0.298012
4.066667	-2.253143	0.495475	0.000088	0.297776
3.956508	-2.283003	0.500480	0.000109	0.297534
4.243903	-2.382415	0.505485	0.000055	0.297304
3.802888	-2.360843	0.510490	0.000138	0.297019
3.743477	-2.400483	0.515494	0.000149	0.296773
3.740261	-2.447920	0.520499	0.000149	0.296538
3.563193	-2.465094	0.525504	0.000182	0.296297
3.269299	-2.454047	0.530509	0.000237	0.296090
3.316772	-2.524173	0.535514	0.000228	0.295789
3.685545	-2.636343	0.540518	0.000160	0.295568
3.200711	-2.597384	0.545523	0.000250	0.295327
3.295363	-2.668096	0.550528	0.000233	0.295065
2.961543	-2.653327	0.555533	0.000295	0.294839
3.226753	-2.759643	0.560538	0.000245	0.294554
2.935813	-2.761768	0.565542	0.000300	0.294283
3.016949	-2.831432	0.570547	0.000285	0.294013
2.855377	-2.854113	0.575552	0.000315	0.293756
2.591324	-2.858449	0.580557	0.000364	0.293498
0.698664	-2.557436	0.585562	0.000716	0.293286
0.455133	-2.569674	0.590566	0.000762	0.293007
0.083016	-2.543250	0.595571	0.000831	0.292803
-0.132294	-2.541966	0.600576	0.000871	0.292616
-0.125186	-2.597086	0.605581	0.000870	0.292349
-0.379345	-2.598647	0.610586	0.000917	0.292113
-0.619298	-2.587179	0.615590	0.000962	0.291953
-1.069812	-2.548033	0.620595	0.001046	0.291741
-1.388290	-2.537919	0.625600	0.001105	0.291504
-1.839536	-2.478714	0.630605	0.001189	0.291390
-2.408394	-2.428425	0.635610	0.001295	0.291126
-2.731638	-2.396248	0.640614	0.001355	0.290994
-2.761853	-2.429967	0.645619	0.001361	0.290798
-3.068024	-2.410429	0.650624	0.001418	0.290618
-2.848178	-2.466034	0.655629	0.001377	0.290540
-2.841412	-2.539514	0.660634	0.001376	0.290180
-3.226144	-2.486668	0.665638	0.001448	0.290095
-3.609872	-2.460563	0.670643	0.001519	0.289877
-4.563046	-2.318827	0.675648	0.001697	0.289719
-4.551806	-2.353112	0.680653	0.001695	0.289558
-4.483190	-2.401052	0.685658	0.001682	0.289380
-4.855978	-2.356993	0.690662	0.001751	0.289261
-4.898012	-2.395281	0.695667	0.001759	0.289031
-5.062550	-2.388408	0.700672	0.001790	0.288916
-5.275240	-2.394757	0.705677	0.001829	0.288690
-5.833919	-2.307520	0.710682	0.001933	0.288618
-5.942966	-2.338778	0.715686	0.001954	0.288361
-6.255405	-2.293105	0.720691	0.002012	0.288305
-6.643212	-2.267308	0.725696	0.002084	0.288081
-6.111194	-2.380581	0.730701	0.001985	0.287997
-6.473213	-2.357429	0.735706	0.002053	0.287783
-6.657594	-2.347642	0.740710	0.002087	0.287663
-6.621919	-2.392875	0.745715	0.002081	0.287468
-6.768883	-2.393893	0.750720	0.002108	0.287328
-6.917156	-2.402496	0.755725	0.002136	0.287149
-7.597457	-2.303145	0.760730	0.002262	0.287026
-7.886835	-2.274302	0.765734	0.002316	0.286906
-7.822334	-2.318097	0.770739	0.002304	0.286744
-8.436051	-2.220620	0.775744	0.002418	0.286672
-8.558408	-2.249812	0.780749	0.002441	0.286412
-8.598485	-2.242831	0.785754	0.002449	0.286411
-9.336879	-2.158949	0.790758	0.002586	0.286156
-8.953056	-2.241138	0.795763	0.002515	0.286093
-9.209070	-2.219874	0.800768	0.002563	0.285965
-9.278589	-2.242218	0.805773	0.002576	0.285788
-9.514260	-2.202088	0.810778	0.002619	0.285774
-9.763399	-2.204711	0.815782	0.002666	0.285531
-9.729226	-2.208186	0.820787	0.002660	0.285544
-10.016950	-2.195085	0.825792	0.002713	0.285345
-10.311207	-2.170111	0.830797	0.002768	0.285200
-10.143616	-2.208057	0.835802	0.002737	0.285162
-10.807645	-2.141337	0.840806	0.002861	0.284888
-11.111472	-2.084166	0.845811	0.002917	0.284897
-10.865127	-2.159958	0.850816	0.002871	0.284740
-10.972369	-2.175798	0.855821	0.002891	0.284560
-11.169797	-2.141296	0.860826	0.002928	0.284552
-11.839859	-2.063153	0.865830	0.003053	0.284330
-12.088957	-2.023053	0.870835	0.003099	0.284303
-12.563217	-1.938053	0.875840	0.003188	0.284297
-12.584495	-1.991143	0.880845	0.003192	0.284007
-12.287666	-2.055756	0.885850	0.003136	0.283952
-12.421401	-2.032088	0.890854	0.003161	0.283949
-12.658667	-2.047487	0.895859	0.003206	0.283650
-12.702869	-2.042615	0.900864	0.003214	0.283634
-12.669482	-2.057276	0.905869	0.003208	0.283589
-13.710846	-1.917388	0.910874	0.003402	0.283337
-13.696031	-1.919657	0.915878	0.003399	0.283339
-13.739289	-1.907303	0.920883	0.003407	0.283361
-14.324499	-1.859823	0.925888	0.003516	0.283060
-14.275558	-1.868351	0.930893	0.003507	0.283062
-14.110409	-1.899110	0.935898	0.003476	0.283058
-13.913301	-1.985294	0.940902	0.003439	0.282800
-13.936660	-2.003259	0.945907	0.003444	0.282686
-13.883255	-2.015014	0.950912	0.003434	0.282676
-13.622939	-2.109901	0.955917	0.003386	0.282432
-14.061526	-2.044637	0.960922	0.003467	0.282357
-13.819775	-2.099126	0.965926	0.003422	0.282303
-13.978886	-2.121226	0.970931	0.003452	0.282041
-14.866837	-1.957859	0.975936	0.003617	0.282051
-14.957654	-1.958045	0.980941	0.003634	0.281965
-15.070172	-1.976427	0.985946	0.003655	0.281765
-15.056465	-1.978364	0.990950	0.003653	0.281768
-15.484348	-1.923006	0.995955	0.003732	0.281652
-16.072713	-1.857016	1.000960	0.003842	0.281441
-15.316476	-1.994860	1.005965	0.003701	0.281439
-15.492019	-1.985763	1.010970	0.003734	0.281322
-16.415549	-1.853541	1.015974	0.003906	0.281138
-15.750074	-1.975004	1.020979	0.003782	0.281135
-15.443381	-2.058315	1.025984	0.003725	0.280993
-16.055570	-1.983978	1.030989	0.003839	0.280802
-15.722806	-2.047855	1.035994	0.003777	0.280785
-15.852594	-2.053455	1.040998	0.003801	0.280634
-15.841765	-2.071614	1.046003	0.003799	0.280550
-16.068650	-2.030646	1.051008	0.003842	0.280549
-15.865409	-2.134161	1.056013	0.003804	0.280205
-16.221925	-2.070188	1.061018	0.003870	0.280200
-16.746724	-1.997554	1.066022	0.003968	0.280082
-16.495245	-2.078888	1.071027	0.003921	0.279898
-16.589526	-2.064305	1.076032	0.003939	0.279884
-16.821118	-2.068836	1.081037	0.003982	0.279643
-17.257928	-2.004310	1.086042	0.004063	0.279566
-17.276900	-2.001541	1.091046	0.004067	0.279562
-17.803567	-1.956639	1.096051	0.004165	0.279298
-18.198710	-1.883864	1.101056	0.004239	0.279303
-17.977337	-1.924741	1.106061	0.004197	0.279299
-18.070781	-1.973641	1.111066	0.004215	0.278957
-18.330063	-1.926079	1.116070	0.004263	0.278959
-18.275140	-1.941099	1.121075	0.004253	0.278933
-18.527232	-1.951300	1.126080	0.004300	0.278642
-18.145299	-2.022904	1.131085	0.004229	0.278630
-18.677678	-1.940368	1.136090	0.004328	0.278556
-18.265974	-2.063391	1.141094	0.004252	0.278305
-17.969133	-2.118234	1.146099	0.004196	0.278301
-18.768138	-2.009880	1.151104	0.004345	0.278108
-18.559279	-2.066226	1.156109	0.004306	0.278012
-19.045072	-1.975527	1.161114	0.004397	0.278025
-19.616924	-1.934508	1.166118	0.004503	0.277696
-19.278831	-1.995994	1.171123	0.004440	0.277696
-19.315978	-2.004349	1.176128	0.004447	0.277617
-19.993335	-1.924730	1.181133	0.004573	0.277390
-19.811800	-1.960610	1.186138	0.004540	0.277374
-19.580769	-2.028892	1.191142	0.004497	0.277237
-20.210250	-1.948620	1.196147	0.004614	0.277058
-20.671802	-1.863955	1.201152	0.004700	0.277062
-20.014641	-2.009253	1.206157	0.004578	0.276927
-20.351871	-1.979923	1.211162	0.004641	0.276759
-20.464165	-1.961370	1.216166	0.004661	0.276749
-20.427999	-2.010241	1.221171	0.004655	0.276528
-20.651176	-1.990079	1.226176	0.004696	0.276421
-20.537890	-2.014351	1.231181	0.004675	0.276401
-21.257174	-1.935576	1.236186	0.004809	0.276128
-21.351196	-1.918353	1.241190	0.004827	0.276129
-21.153437	-1.965790	1.246195	0.004790	0.276069
-22.043197	-1.852217	1.251200	0.004956	0.275815
-21.702065	-1.911819	1.256205	0.004892	0.275828
-21.548964	-1.952650	1.261210	0.004864	0.275759
-21.964956	-1.913353	1.266214	0.004941	0.275568
-21.971392	-1.908816	1.271219	0.004942	0.275586
-22.161637	-1.900188	1.276224	0.004978	0.275449
-22.375587	-1.901987	1.281229	0.005018	0.275235
-22.497154	-1.880056	1.286234	0.005040	0.275234
-22.123833	-1.980095	1.291238	0.004971	0.275064
-22.137953	-2.007000	1.296243	0.004974	0.274909
-22.713623	-1.904009	1.301248	0.005081	0.274900
-22.525495	-1.986187	1.306253	0.005046	0.274647
-22.338471	-2.035459	1.311258	0.005011	0.274566
-22.972866	-1.926641	1.316262	0.005129	0.274532
-23.687665	-1.838088	1.321267	0.005262	0.274313
-23.359555	-1.900927	1.326272	0.005201	0.274296
-23.026597	-1.980980	1.331277	0.005140	0.274193
-23.759540	-1.891910	1.336282	0.005276	0.273959
-23.478066	-1.944541	1.341286	0.005224	0.273951
-23.408156	-1.988064	1.346291	0.005211	0.273788
-24.365477	-1.840106	1.351296	0.005389	0.273649
-23.856662	-1.931538	1.356301	0.005294	0.273655
-24.030289	-1.943847	1.361306	0.005327	0.273422
-24.551281	-1.866228	1.366310	0.005424	0.273332
-24.508842	-1.871435	1.371315	0.005416	0.273345
-24.621472	-1.901072	1.376320	0.005437	0.273079
-24.891411	-1.855209	1.381325	0.005487	0.273062
-25.246289	-1.791495	1.386330	0.005553	0.273057
-24.976254	-1.902920	1.391334	0.005503	0.272726
-24.737260	-1.950127	1.396339	0.005459	0.272706
-25.383929	-1.841176	1.401344	0.005579	0.272660
-25.359393	-1.896311	1.406349	0.005574	0.272390
-25.470713	-1.875292	1.411354	0.005595	0.272394
-25.110815	-1.965164	1.416358	0.005528	0.272264
-25.738144	-1.887895	1.421363	0.005645	0.272068
-25.621816	-1.911055	1.426368	0.005623	0.272057
-25.766279	-1.913742	1.431373	0.005650	0.271903
-26.102509	-1.876321	1.436378	0.005713	0.271776
-26.075533	-1.882031	1.441382	0.005708	0.271772
-25.409953	-2.056116	1.446387	0.005584	0.271489
-26.548532	-1.858305	1.451392	0.005796	0.271439
-26.063210	-1.960942	1.456397	0.005706	0.271362
-25.868583	-2.043614	1.461402	0.005670	0.271110
-26.263538	-1.970566	1.466406	0.005743	0.271116
-26.697433	-1.928315	1.471411	0.005824	0.270920
-27.129786	-1.868298	1.476416	0.005905	0.270820
-27.039568	-1.881208	1.481421	0.005888	0.270839
-27.344074	-1.873514	1.486426	0.005945	0.270584
-27.755527	-1.800469	1.491430	0.006021	0.270574
-27.188207	-1.908030	1.496435	0.005916	0.270550
-27.556075	-1.903390	1.501440	0.005984	0.270216
-27.902537	-1.837731	1.506445	0.006049	0.270230
-27.925398	-1.850351	1.511450	0.006053	0.270140
-28.290730	-1.825861	1.516454	0.006121	0.269915
-27.947436	-1.889060	1.521459	0.006057	0.269911
-28.079638	-1.897402	1.526464	0.006082	0.269737
-28.598735	-1.829590	1.531469	0.006179	0.269594
-28.118284	-1.921596	1.536474	0.006089	0.269569
-28.675090	-1.858597	1.541478	0.006193	0.269363
-28.455708	-1.910676	1.546483	0.006152	0.269297
-28.630868	-1.883565	1.551488	0.006185	0.269271
-28.981110	-1.877628	1.556493	0.006250	0.268960
-29.037371	-1.866754	1.561498	0.006260	0.268964
-28.987560	-1.899491	1.566502	0.006251	0.268836
-29.700905	-1.801292	1.571507	0.006384	0.268666
-29.877365	-1.769632	1.576512	0.006417	0.268663
-29.576901	-1.849267	1.581517	0.006361	0.268528
-30.021194	-1.804357	1.586522	0.006444	0.268334
-30.293031	-1.755088	1.591526	0.006494	0.268333
-29.800359	-1.873150	1.596531	0.006403	0.268179
-29.957286	-1.872151	1.601536	0.006432	0.268030
-29.759404	-1.908057	1.606541	0.006395	0.268031
-29.984662	-1.925608	1.611546	0.006437	0.267714
-29.798128	-1.966098	1.616550	0.006403	0.267678
-29.789782	-1.991158	1.621555	0.006401	0.267551
-30.495616	-1.896594	1.626560	0.006533	0.267368
-30.682954	-1.857905	1.631565	0.006567	0.267392
-30.781380	-1.892157	1.636570	0.006586	0.267110
-31.110853	-1.843109	1.641574	0.006647	0.267050
-30.431390	-1.977287	1.646579	0.006521	0.266993
-31.386326	-1.844681	1.651584	0.006699	0.266770
-31.631764	-1.796864	1.656589	0.006744	0.266787
-31.380874	-1.870732	1.661594	0.006698	0.266633
-31.740481	-1.842418	1.666598	0.006765	0.266431
-31.666709	-1.853582	1.671603	0.006751	0.266443
-31.715496	-1.889838	1.676608	0.006760	0.266198
-32.015268	-1.846034	1.681613	0.006816	0.266139
-32.239458	-1.805808	1.686618	0.006858	0.266136
-32.788118	-1.762709	1.691622	0.006960	0.265827
-32.027914	-1.903846	1.696627	0.006818	0.265811
-32.035887	-1.920315	1.701632	0.006820	0.265713
-32.282013	-1.907844	1.706637	0.006866	0.265537
-32.516458	-1.862784	1.711642	0.006909	0.265550
-32.629265	-1.890111	1.716646	0.006931	0.265289
-32.880876	-1.858097	1.721651	0.006977	0.265213
-33.198859	-1.806188	1.726656	0.007037	0.265181
-33.098350	-1.877354	1.731661	0.007018	0.264892
-33.209784	-1.857506	1.736666	0.007039	0.264889
-33.336751	-1.864264	1.741670	0.007062	0.264726
-33.431011	-1.876475	1.746675	0.007080	0.264565
-33.379217	-1.888014	1.751680	0.007070	0.264553
-33.761143	-1.860323	1.756685	0.007142	0.264324
-33.966812	-1.831309	1.761690	0.007180	0.264278
-33.823931	-1.867685	1.766694	0.007153	0.264221
-33.827611	-1.917157	1.771699	0.007154	0.263945
-34.137422	-1.864460	1.776704	0.007212	0.263925
-34.388856	-1.849260	1.781709	0.007259	0.263757
-34.530343	-1.845142	1.786714	0.007285	0.263638
-34.782436	-1.798890	1.791718	0.007332	0.263640
-34.870255	-1.836221	1.796723	0.007348	0.263347
-35.106758	-1.798035	1.801728	0.007392	0.263320
-35.039510	-1.821853	1.806733	0.007380	0.263256
-35.012707	-1.869645	1.811738	0.007375	0.263020
-35.006511	-1.872019	1.816742	0.007374	0.263013
-35.368264	-1.840712	1.821747	0.007441	0.262823
-35.682494	-1.810875	1.826752	0.007500	0.262672
-35.640427	-1.814748	1.831757	0.007492	0.262692
-35.622054	-1.871910	1.836762	0.007489	0.262395
-36.148424	-1.780554	1.841766	0.007587	0.262371
-35.734475	-1.873361	1.846771	0.007510	0.262274
-35.949752	-1.876213	1.851776	0.007550	0.262042
-35.847973	-1.896811	1.856781	0.007531	0.262030
-36.287446	-1.855326	1.861786	0.007613	0.261817
-36.086837	-1.906660	1.866790	0.007576	0.261735
-35.728563	-1.989175	1.871795	0.007509	0.261639
-36.135597	-1.960544	1.876800	0.007585	0.261387
-36.445974	-1.899577	1.881805	0.007643	0.261412
-36.684253	-1.903952	1.886810	0.007687	0.261147
-37.189485	-1.819384	1.891814	0.007781	0.261106
-37.155439	-1.840708	1.896819	0.007775	0.261022
-37.636058	-1.793027	1.901824	0.007864	0.260801
-37.186883	-1.877210	1.906829	0.007781	0.260787
-37.427450	-1.860681	1.911834	0.007825	0.260635
-37.601287	-1.844827	1.916838	0.007858	0.260548
-37.664300	-1.834019	1.921843	0.007870	0.260544
-38.161878	-1.802885	1.926848	0.007962	0.260213
-37.800926	-1.868282	1.931853	0.007895	0.260214
-37.410259	-1.970816	1.936858	0.007823	0.260039
-38.309496	-1.835047	1.941862	0.007990	0.259884
-38.248962	-1.843748	1.946867	0.007979	0.259896
-38.581103	-1.842560	1.951872	0.008041	0.259566
-38.554763	-1.846194	1.956877	0.008036	0.259572
-38.819583	-1.820311	1.961882	0.008085	0.259447
-39.441890	-1.733217	1.966886	0.008201	0.259301
-39.048716	-1.803689	1.971891	0.008128	0.259307
-39.147036	-1.832669	1.976896	0.008146	0.259045
-39.752540	-1.737254	1.981901	0.008259	0.258962
-39.287418	-1.826539	1.986906	0.008172	0.258936
-39.834556	-1.780545	1.991910	0.008274	0.258636
-39.805222	-1.782386	1.996915	0.008269	0.258655
-39.497892	-1.880320	2.001920	0.008212	0.258420

-40.064293	-1.809698	2.011917	0.008317	0.258238
-39.846421	-1.886758	2.021914	0.008277	0.258027
-39.985901	-1.905228	2.031910	0.008303	0.257780
-40.539924	-1.818682	2.041907	0.008406	0.257700
-40.606208	-1.856673	2.051904	0.008418	0.257418
-40.655633	-1.856582	2.061901	0.008428	0.257368
-40.703361	-1.878720	2.071898	0.008437	0.257194
-40.655852	-1.916175	2.081894	0.008428	0.257031
-40.991236	-1.852916	2.091891	0.008491	0.257043
-40.821472	-1.903998	2.101888	0.008459	0.256929
-41.508451	-1.809989	2.111885	0.008587	0.256754
-41.136423	-1.877095	2.121882	0.008518	0.256756
-41.496145	-1.809589	2.131878	0.008585	0.256768
-41.524131	-1.804426	2.141875	0.008590	0.256768
-41.594616	-1.790558	2.151872	0.008603	0.256773
-41.582785	-1.795518	2.161869	0.008601	0.256757
-40.923352	-1.915653	2.171866	0.008479	0.256755
-41.235295	-1.858655	2.181862	0.008537	0.256756
-41.230547	-1.858191	2.191859	0.008536	0.256763
-41.029308	-1.896918	2.201856	0.008499	0.256751
-41.328070	-1.841743	2.211853	0.008554	0.256755
-41.085583	-1.874851	2.221850	0.008509	0.256817
-40.852548	-1.877250	2.231846	0.008466	0.257042
-40.778138	-1.890630	2.241843	0.008452	0.257042
-40.700032	-1.906909	2.251840	0.008438	0.257030
-40.971454	-1.855466	2.261837	0.008488	0.257041
-40.497223	-1.917866	2.271834	0.008400	0.257176
-40.652342	-1.854416	2.281830	0.008429	0.257373
-40.699542	-1.847278	2.291827	0.008438	0.257365
-40.678984	-1.831256	2.301824	0.008434	0.257476
-40.212734	-1.880569	2.311821	0.008347	0.257675
-40.073674	-1.905833	2.321818	0.008322	0.257675
-40.308781	-1.830785	2.331814	0.008365	0.257856
-40.256167	-1.807621	2.341811	0.008356	0.258039
-39.813647	-1.880348	2.351808	0.008273	0.258082
-39.418407	-1.914605	2.361805	0.008200	0.258293
-38.703527	-2.047658	2.371802	0.008067	0.258276
-39.209348	-1.916240	2.381798	0.008161	0.258496
-39.162958	-1.902305	2.391795	0.008153	0.258621
-39.098800	-1.886942	2.401792	0.008141	0.258772
-38.913498	-1.891835	2.411789	0.008106	0.258933
-38.753906	-1.892337	2.421786	0.008077	0.259092
-38.576599	-1.893173	2.431782	0.008044	0.259267
-38.774440	-1.823061	2.441779	0.008081	0.259457
-38.732599	-1.811429	2.451776	0.008073	0.259564
-38.179061	-1.859419	2.461773	0.007970	0.259858
-37.880700	-1.900922	2.471770	0.007914	0.259928
-37.576017	-1.908565	2.481766	0.007858	0.260194
-37.232620	-1.951607	2.491763	0.007794	0.260302
-36.612065	-2.024873	2.501760	0.007678	0.260522
-36.619255	-2.009480	2.511757	0.007680	0.260600
-36.595755	-1.983511	2.521754	0.007676	0.260767
-36.370704	-1.995178	2.531750	0.007634	0.260929
-36.353557	-1.968569	2.541747	0.007631	0.261094
-36.237602	-1.944617	2.551744	0.007609	0.261343
-36.010448	-1.966150	2.561741	0.007567	0.261452
-36.198873	-1.879022	2.571738	0.007602	0.261744
-35.861952	-1.908700	2.581734	0.007539	0.261919
-35.723451	-1.904361	2.591731	0.007514	0.262082
-35.871849	-1.825634	2.601728	0.007541	0.262367
-34.969969	-1.949942	2.611725	0.007374	0.262586
-35.111547	-1.895666	2.621722	0.007400	0.262743
-34.681068	-1.925063	2.631718	0.007320	0.263012
-34.448160	-1.930644	2.641715	0.007277	0.263214
-34.424681	-1.905984	2.651712	0.007272	0.263373
-33.733634	-1.987921	2.661709	0.007144	0.263613
-33.652641	-1.962543	2.671706	0.007129	0.263832
-33.198923	-2.020365	2.681702	0.007044	0.263968
-33.621344	-1.886894	2.691699	0.007123	0.264278
-34.062152	-1.763248	2.701696	0.007205	0.264515
-33.730416	-1.777925	2.711693	0.007143	0.264765
-33.428986	-1.789141	2.721690	0.007087	0.265003
-32.812302	-1.863276	2.731686	0.006973	0.265210
-32.464911	-1.865068	2.741683	0.006908	0.265545
-32.095404	-1.901236	2.751680	0.006839	0.265714
-32.063126	-1.875124	2.761677	0.006833	0.265888
-31.856694	-1.870008	2.771674	0.006795	0.266119
-31.542022	-1.871276	2.781670	0.006737	0.266423
-31.621347	-1.813473	2.791667	0.006751	0.266659
-31.366385	-1.818989	2.801664	0.006704	0.266880
-31.192356	-1.810819	2.811661	0.006672	0.267096
-30.703258	-1.846882	2.821658	0.006581	0.267382
-30.242354	-1.883743	2.831654	0.006495	0.267636
-29.902646	-1.908135	2.841651	0.006432	0.267837
-29.567300	-1.931137	2.851648	0.006369	0.268042
-29.050415	-1.977805	2.861645	0.006273	0.268298
-29.214077	-1.909428	2.871642	0.006304	0.268505
-28.562294	-1.992992	2.881638	0.006183	0.268694
-28.858561	-1.892678	2.891635	0.006238	0.268943
-28.796003	-1.844465	2.901632	0.006226	0.269264
-28.885461	-1.787526	2.911629	0.006243	0.269482
-28.608703	-1.792904	2.921626	0.006191	0.269723
-28.185673	-1.823526	2.931622	0.006113	0.269971
-27.954507	-1.814761	2.941619	0.006070	0.270243
-28.020030	-1.744227	2.951616	0.006082	0.270556
-27.637079	-1.772997	2.961613	0.006011	0.270775
-26.998813	-1.850531	2.971610	0.005892	0.270980
-26.790052	-1.845400	2.981606	0.005853	0.271210
-26.346528	-1.884702	2.991603	0.005771	0.271430
-26.203619	-1.852469	3.001600	0.005744	0.271740
-25.979918	-1.854385	3.011597	0.005703	0.271946
-25.221071	-1.959821	3.021594	0.005562	0.272119
-24.706412	-2.007651	3.031590	0.005466	0.272362
-25.102365	-1.886343	3.041587	0.005540	0.272624
-25.094736	-1.841412	3.051584	0.005538	0.272869
-24.377057	-1.933798	3.061581	0.005405	0.273071
-24.448217	-1.871323	3.071578	0.005418	0.273333
-24.064490	-1.891350	3.081574	0.005347	0.273596
-23.770223	-1.907948	3.091571	0.005292	0.273791
-23.661912	-1.886401	3.101568	0.005272	0.274009
-23.196059	-1.920683	3.111565	0.005185	0.274275
-22.985679	-1.909935	3.121562	0.005146	0.274533
-22.894840	-1.885101	3.131558	0.005129	0.274751
-22.760909	-1.868087	3.141555	0.005104	0.274968
-22.601052	-1.846736	3.151552	0.005075	0.275233
-22.483029	-1.808233	3.161549	0.005053	0.275548
-22.210911	-1.819264	3.171546	0.005002	0.275750
-22.037659	-1.808429	3.181542	0.004970	0.275971
-21.491124	-1.866846	3.191539	0.004868	0.276186
-21.239314	-1.865238	3.201536	0.004822	0.276434
-21.473436	-1.762625	3.211533	0.004865	0.276748
-21.034625	-1.796129	3.221530	0.004784	0.276989
-21.048816	-1.743934	3.231526	0.004786	0.277248
-20.188253	-1.857693	3.241523	0.004626	0.277471
-20.097607	-1.828377	3.251520	0.004609	0.277709
-19.719379	-1.834358	3.261517	0.004539	0.278036
-19.190527	-1.891905	3.271514	0.004441	0.278237
-19.222808	-1.845463	3.281510	0.004447	0.278447
-18.624871	-1.916319	3.291507	0.004336	0.278644
-18.457415	-1.887257	3.301504	0.004304	0.278952
-18.201344	-1.891722	3.311501	0.004257	0.279170
-17.673763	-1.952519	3.321498	0.004159	0.279352
-17.797222	-1.886671	3.331494	0.004182	0.279576
-17.180062	-1.940999	3.341491	0.004067	0.279875
-17.405965	-1.860653	3.351488	0.004109	0.280078
-17.332608	-1.828833	3.361485	0.004095	0.280311
-16.894252	-1.857619	3.371482	0.004014	0.280573
-16.477033	-1.891790	3.381478	0.003936	0.280788
-16.018366	-1.938759	3.391475	0.003851	0.280975
-15.780150	-1.943969	3.401472	0.003807	0.281171
-15.481405	-1.951821	3.411469	0.003751	0.281410
-14.901354	-2.007748	3.421466	0.003643	0.281664
-15.346481	-1.887656	3.431462	0.003726	0.281865
-14.962285	-1.920059	3.441459	0.003655	0.282057
-15.027796	-1.846138	3.451456	0.003667	0.282375
-14.610978	-1.877404	3.461453	0.003589	0.282602
-14.916172	-1.771133	3.471450	0.003646	0.282862
-14.069908	-1.883004	3.481446	0.003489	0.283076
-13.815921	-1.882400	3.491443	0.003442	0.283315
-13.498282	-1.885692	3.501440	0.003383	0.283593
-12.996461	-1.940645	3.511437	0.003289	0.283778
-12.895631	-1.919659	3.521434	0.003271	0.283978
-12.560764	-1.923162	3.531430	0.003208	0.284270
-12.164888	-1.952597	3.541427	0.003135	0.284486
-12.683990	-1.812374	3.551424	0.003231	0.284718
-12.298052	-1.836500	3.561421	0.003160	0.284952
-12.040223	-1.830056	3.571418	0.003112	0.285222
-12.022655	-1.771073	3.581414	0.003108	0.285537
-10.973789	-1.930017	3.591411	0.002913	0.285698
-10.640099	-1.961343	3.601408	0.002851	0.285846
-10.487384	-1.936978	3.611405	0.002823	0.286109
-10.202961	-1.939493	3.621402	0.002770	0.286358
-9.979154	-1.941367	3.631398	0.002728	0.286554
-9.664520	-1.959133	3.641395	0.002670	0.286752
-9.632011	-1.909199	3.651392	0.002664	0.287034
-9.594655	-1.874358	3.661389	0.002657	0.287243
-9.708200	-1.804381	3.671386	0.002678	0.287491
-8.872372	-1.914527	3.681382	0.002523	0.287701
-8.666629	-1.885749	3.691379	0.002484	0.288034
-8.438679	-1.888333	3.701376	0.002442	0.288228
-8.294550	-1.873974	3.711373	0.002415	0.288432
-7.830538	-1.918260	3.721370	0.002329	0.288632
-7.489627	-1.919868	3.731366	0.002266	0.288934
-6.940163	-1.983192	3.741363	0.002163	0.289117
-7.151094	-1.904621	3.751360	0.002203	0.289318
-6.689934	-1.938717	3.761357	0.002117	0.289566
-6.051292	-2.013132	3.771354	0.001998	0.289774
-6.142236	-1.958685	3.781350	0.002015	0.289963
-6.048768	-1.926240	3.791347	0.001998	0.290209
-6.181194	-1.840132	3.801344	0.002023	0.290518
-6.119687	-1.812135	3.811341	0.002011	0.290713
-5.969011	-1.795687	3.821338	0.001983	0.290930
-5.254820	-1.883414	3.831334	0.001850	0.291139
-4.830167	-1.901976	3.841331	0.001771	0.291430
-5.048938	-1.813284	3.851328	0.001812	0.291673
-4.614877	-1.849554	3.861325	0.001731	0.291884
-4.158121	-1.894772	3.871322	0.001646	0.292071
-4.334920	-1.797902	3.881318	0.001679	0.292391
-3.832538	-1.840791	3.891315	0.001586	0.292630
-3.676910	-1.824595	3.901312	0.001557	0.292850
-3.657181	-1.780439	3.911309	0.001553	0.293085
-3.559941	-1.749355	3.921306	0.001535	0.293325
-3.484341	-1.697102	3.931302	0.001521	0.293651
-3.079631	-1.721077	3.941299	0.001446	0.293894
-2.601868	-1.758499	3.951296	0.001357	0.294137
-2.620795	-1.705941	3.961293	0.001361	0.294378
-2.718835	-1.634655	3.971290	0.001379	0.294641
-2.570640	-1.602471	3.981286	0.001352	0.294931
-2.052542	-1.638817	3.991283	0.001255	0.295214
-2.399123	-1.510229	4.001280	0.001320	0.295535
-2.592611	-1.424768	4.011277	0.001356	0.295781
-2.282713	-1.419643	4.021274	0.001298	0.296081
-2.243344	-1.363180	4.031270	0.001291	0.296391
-1.879072	-1.363371	4.041267	0.001223	0.296713
-1.712502	-1.334983	4.051264	0.001192	0.296998
-1.784378	-1.253427	4.061261	0.001206	0.297332
-1.665881	-1.207010	4.071258	0.001184	0.297662
-1.428760	-1.178579	4.081254	0.001139	0.298009
-1.319826	-1.129270	4.091251	0.001119	0.298344
-1.333407	-1.054663	4.101248	0.001122	0.298693
-1.145401	-1.015237	4.111245	0.001087	0.299049
-0.913644	-0.985084	4.121242	0.001044	0.299398
-0.614926	-0.968120	4.131238	0.000988	0.299742
-0.546448	-0.906504	4.141235	0.000975	0.300099
-0.889474	-0.763026	4.151232	0.001039	0.300490
-1.072064	-0.650968	4.161229	0.001073	0.300869
-1.209604	-0.540597	4.171226	0.001099	0.301279
-0.344709	-0.619798	4.181222	0.000938	0.301653
-0.530495	-0.500521	4.191219	0.000973	0.302062
-0.560499	-0.403994	4.201216	0.000978	0.302498
-0.466731	-0.333628	4.211213	0.000961	0.302915
-0.285077	-0.276069	4.221210	0.000927	0.303347
-0.201120	-0.199109	4.231206	0.000911	0.303787
0.275211	-0.202183	4.241203	0.000823	0.304184
0.459325	-0.138227	4.251200	0.000789	0.304646
0.647388	-0.087066	4.261197	0.000754	0.305051
0.697333	0.001919	4.271194	0.000744	0.305515
0.588248	0.112911	4.281190	0.000765	0.305946
0.410398	0.242209	4.291187	0.000798	0.306404
0.000000	0.418184	4.301184	0.000874	0.306883

0.435858	0.600303	4.306189	0.000793	0.308112
1.003830	1.045616	4.311194	0.000687	0.310677
1.301358	1.832846	4.316198	0.000631	0.314571
1.299380	2.959195	4.321203	0.000631	0.319708
1.088845	4.410502	4.326208	0.000669	0.326041
1.435596	6.051971	4.331213	0.000603	0.333519
1.238522	8.086899	4.336218	0.000639	0.342082
1.328184	10.383062	4.341222	0.000621	0.351728
1.874716	12.887674	4.346227	0.000517	0.362281
2.183645	15.758389	4.351232	0.000458	0.373787
2.243343	19.008778	4.356237	0.000445	0.386205
2.571733	22.528043	4.361242	0.000381	0.399388
3.224150	26.335827	4.366246	0.000257	0.413366
3.316705	30.593693	4.371251	0.000237	0.428067
3.854098	35.103025	4.376256	0.000134	0.443364
4.326302	39.989176	4.381261	0.000043	0.459302
4.483904	45.267720	4.386266	0.000011	0.475726
4.853556	50.854912	4.391270	-0.000062	0.492621
5.506014	56.733931	4.396275	-0.000187	0.509929
6.635020	62.853786	4.401280	-0.000401	0.527565
6.730723	69.498212	4.406285	-0.000423	0.545528
6.604981	76.484408	4.411290	-0.000404	0.563693
7.820952	83.532761	4.416294	-0.000635	0.582046
8.323538	90.992127	4.421299	-0.000734	0.600518
9.328905	98.628538	4.426304	-0.000926	0.619062
10.858991	106.441202	4.431309	-0.001216	0.637680
11.222812	114.703230	4.436314	-0.001289	0.656299
12.185040	123.074250	4.441318	-0.001474	0.674866
13.105600	131.641819	4.446323	-0.001651	0.693330
13.803854	140.431856	4.451328	-0.001786	0.711686
14.793390	149.333561	4.456333	-0.001976	0.729904
15.950728	158.339617	4.461338	-0.002198	0.747936
17.032272	167.492194	4.466342	-0.002405	0.765795
17.991051	176.773933	4.471347	-0.002589	0.783443
19.194101	186.091662	4.476352	-0.002819	0.800845
19.730890	195.631871	4.481357	-0.002926	0.818061
20.399864	205.204963	4.486362	-0.003056	0.835019
21.423318	214.719209	4.491366	-0.003253	0.851645
22.193327	224.318412	4.496371	-0.003403	0.868019
22.945991	233.925754	4.501376	-0.003549	0.884097
23.789168	243.539028	4.506381	-0.003712	0.899923
24.777002	253.106702	4.511386	-0.003902	0.915443
25.447825	262.720736	4.516390	-0.004034	0.930688
25.864296	272.366027	4.521395	-0.004117	0.945667
26.581688	281.908482	4.526400	-0.004257	0.960337
27.465124	291.417364	4.531405	-0.004428	0.974779
28.334521	300.874965	4.536410	-0.004596	0.988930
28.952649	310.347677	4.541414	-0.004717	1.002840
29.829277	319.720892	4.546419	-0.004886	1.016482
31.065054	328.988611	4.551424	-0.005122	1.029882
31.916615	338.291069	4.556429	-0.005287	1.043065
32.533107	347.596857	4.561434	-0.005408	1.056031
33.607213	356.784385	4.566438	-0.005614	1.068787
34.508678	365.940338	4.571443	-0.005787	1.081310
35.422825	375.061749	4.576448	-0.005964	1.093646
36.101165	384.208572	4.581453	-0.006096	1.105824
36.974022	393.234950	4.586458	-0.006264	1.117756
37.812137	402.251287	4.591462	-0.006426	1.129541
38.832753	411.189811	4.596467	-0.006622	1.141145
39.718692	420.127660	4.601472	-0.006793	1.152603
40.477975	429.030269	4.606477	-0.006940	1.163876
40.486849	438.029027	4.611482	-0.006947	1.175001
41.235118	446.839154	4.616486	-0.007092	1.185945
41.871755	455.636236	4.621491	-0.007217	1.196750
42.126052	464.469580	4.626496	-0.007270	1.207424
43.444089	473.097954	4.631501	-0.007521	1.217976
44.188466	481.796067	4.636506	-0.007665	1.228403
44.865588	490.482284	4.641510	-0.007797	1.238716
45.576018	499.122681	4.646515	-0.007934	1.248896
46.372363	507.730058	4.651520	-0.008088	1.258972
46.889561	516.387114	4.656525	-0.008190	1.268971
47.259270	525.002560	4.661530	-0.008265	1.278816
47.659454	533.601532	4.666534	-0.008345	1.288574
48.369212	542.138264	4.671539	-0.008482	1.298246
49.372933	550.604267	4.676544	-0.008675	1.307823
49.604977	559.277709	4.681549	-0.008724	1.317415
50.426514	567.676573	4.686554	-0.008882	1.326747
50.812907	576.194406	4.691558	-0.008959	1.336062
51.308374	584.651168	4.696563	-0.009057	1.345267
51.690381	593.121304	4.701568	-0.009134	1.354403
52.325454	601.534495	4.706573	-0.009257	1.363463
52.510374	610.003928	4.711578	-0.009297	1.372442
52.865136	618.425145	4.716582	-0.009369	1.381342
53.376815	626.827019	4.721587	-0.009470	1.390192
53.893637	635.187400	4.726592	-0.009571	1.398944
54.724188	643.482785	4.731597	-0.009731	1.407628
55.038849	651.884867	4.736602	-0.009795	1.416280
55.600068	660.217870	4.741606	-0.009905	1.424850
56.247699	668.549718	4.746611	-0.010031	1.433382
56.915361	676.847603	4.751616	-0.010161	1.441833
57.490450	685.194017	4.756621	-0.010273	1.450268
58.334128	693.461032	4.761626	-0.010436	1.458618
58.664497	701.834510	4.766630	-0.010503	1.466942
59.200584	710.197577	4.771635	-0.010608	1.475243
59.637546	718.477693	4.776640	-0.010695	1.483399
60.721117	726.689977	4.781645	-0.010902	1.491549
60.976920	735.034964	4.786650	-0.010955	1.499650
61.564460	743.317972	4.791654	-0.011069	1.507701
62.229867	751.578834	4.796659	-0.011199	1.515699
62.373972	759.914815	4.801664	-0.011231	1.523646
62.585203	768.252695	4.806669	-0.011276	1.531564
63.430910	776.435829	4.811674	-0.011438	1.539392
63.852462	784.717640	4.816678	-0.011522	1.547209
64.913484	792.884681	4.821683	-0.011725	1.554976
64.866233	801.230719	4.826688	-0.011722	1.562703
64.985926	809.540988	4.831693	-0.011749	1.570384
65.563561	817.755339	4.836698	-0.011862	1.578007
66.837721	825.841450	4.841702	-0.012105	1.585580
67.091671	834.173182	4.846707	-0.012157	1.593189
67.383641	842.409419	4.851712	-0.012217	1.600682
67.772011	850.674696	4.856717	-0.012295	1.608179
68.108617	858.909156	4.861722	-0.012363	1.615607
68.768541	867.110231	4.866726	-0.012491	1.623017
69.146685	875.361296	4.871731	-0.012567	1.630397
69.866042	883.529928	4.876736	-0.012706	1.637719
70.292938	891.723908	4.881741	-0.012791	1.644990
70.946416	899.891691	4.886746	-0.012918	1.652237
70.999139	908.181550	4.891750	-0.012933	1.659475
71.381227	916.372196	4.896755	-0.013009	1.666642
71.723783	924.590742	4.901760	-0.013078	1.673796
72.359873	932.741354	4.906765	-0.013202	1.680901
73.026965	940.900554	4.911770	-0.013332	1.687988
74.008805	949.022186	4.916774	-0.013520	1.695055
74.744081	957.184179	4.921779	-0.013662	1.702094
74.880549	965.451092	4.926784	-0.013693	1.709112
74.767714	973.742024	4.931789	-0.013677	1.716088
74.698268	981.971688	4.936794	-0.013669	1.722991
75.652363	990.035492	4.941798	-0.013852	1.729862
75.645841	998.309621	4.946803	-0.013856	1.736755
75.374770	1006.573797	4.951808	-0.013811	1.743578
76.093979	1014.665119	4.956813	-0.013950	1.750360
75.989655	1022.908560	4.961818	-0.013936	1.757134
77.547250	1030.823857	4.966822	-0.014231	1.763827
77.687440	1039.071272	4.971827	-0.014263	1.770585
78.156284	1047.217208	4.976832	-0.014355	1.777275
78.943155	1055.327581	4.981837	-0.014507	1.783952
78.818495	1063.634549	4.986842	-0.014489	1.790648
79.355860	1071.784250	4.991846	-0.014595	1.797275
79.435429	1079.967658	4.996851	-0.014615	1.803848
80.029960	1088.042019	5.001856	-0.014731	1.810374
81.001087	1096.104845	5.006861	-0.014917	1.816913
81.057777	1104.312791	5.011866	-0.014933	1.823431
81.471336	1112.456854	5.016870	-0.015015	1.829919
82.183261	1120.565128	5.021875	-0.015153	1.836392
82.522123	1128.727557	5.026880	-0.015221	1.842840
83.025340	1136.882421	5.031885	-0.015320	1.849279
83.031725	1145.080416	5.036890	-0.015327	1.855669
84.429176	1153.029456	5.041894	-0.015592	1.862010
84.560102	1161.264800	5.046899	-0.015622	1.868401
84.931500	1169.418280	5.051904	-0.015696	1.874734
85.215499	1177.576263	5.056909	-0.015754	1.881040
85.768705	1185.696494	5.061914	-0.015862	1.887327
86.371846	1193.829753	5.066918	-0.015980	1.893608
86.557454	1201.997934	5.071923	-0.016020	1.899847
87.619545	1210.020612	5.076928	-0.016223	1.906057
87.898065	1218.214748	5.081933	-0.016280	1.912285
88.356163	1226.329996	5.086938	-0.016370	1.918454
88.440165	1234.504370	5.091942	-0.016391	1.924605
88.693981	1242.675946	5.096947	-0.016444	1.930753
89.220724	1250.752131	5.101952	-0.016547	1.936842
89.483442	1258.925385	5.106957	-0.016601	1.942954
90.234613	1266.988586	5.111962	-0.016747	1.949019
90.323510	1275.147304	5.116966	-0.016768	1.955063
90.948675	1283.223139	5.121971	-0.016890	1.961086
91.059214	1291.386777	5.126976	-0.016916	1.967098
91.787573	1299.451675	5.131981	-0.017057	1.973087
91.569457	1307.666830	5.136986	-0.017021	1.979065
92.184582	1315.705141	5.141990	-0.017141	1.984986
92.546332	1323.851500	5.146995	-0.017214	1.990940
92.568089	1332.000970	5.152000	-0.017223	1.996843
93.439616	1340.002035	5.157005	-0.017391	2.002712
94.097088	1348.078726	5.162010	-0.017518	2.008595
94.058289	1356.285554	5.167014	-0.017516	2.014479
94.370702	1364.399563	5.172019	-0.017580	2.020318
94.395322	1372.556321	5.177024	-0.017590	2.026140
94.859643	1380.658080	5.182029	-0.017681	2.031952
94.993561	1388.794603	5.187034	-0.017711	2.037738
95.800438	1396.782527	5.192038	-0.017867	2.043472
96.192945	1404.898766	5.197043	-0.017945	2.049237
96.537240	1413.000182	5.202048	-0.018015	2.054971
97.206464	1421.051777	5.207053	-0.018144	2.060687
97.582589	1429.170226	5.212058	-0.018220	2.066404
97.808666	1437.333037	5.217062	-0.018267	2.072121
97.545149	1445.536591	5.222067	-0.018223	2.077800
98.145534	1453.538687	5.227072	-0.018340	2.083412
99.080923	1461.561137	5.232077	-0.018520	2.089056
99.243485	1469.697031	5.237082	-0.018555	2.094686
99.645610	1477.803021	5.242086	-0.018635	2.100303
100.193811	1485.871300	5.247091	-0.018743	2.105895
100.457677	1494.028816	5.252096	-0.018797	2.111504
100.883819	1502.135012	5.257101	-0.018882	2.117079
101.812251	1510.116904	5.262106	-0.019060	2.122605
102.073117	1518.255827	5.267110	-0.019113	2.128156
102.545237	1526.347154	5.272115	-0.019207	2.133682
102.735077	1534.469793	5.277120	-0.019247	2.139187
103.178246	1542.535254	5.282125	-0.019335	2.144664
103.675167	1550.617673	5.287130	-0.019433	2.150144
104.071024	1558.705082	5.292134	-0.019512	2.155603
104.038387	1566.888129	5.297139	-0.019511	2.161070
104.607466	1574.899021	5.302144	-0.019622	2.166467
105.445325	1582.925460	5.307149	-0.019783	2.171886
105.738333	1591.067189	5.312154	-0.019843	2.177317
106.138441	1599.149022	5.317158	-0.019923	2.182704
107.000445	1607.200688	5.322163	-0.020088	2.188101
107.353617	1615.310673	5.327168	-0.020159	2.193476
107.756796	1623.424442	5.332173	-0.020240	2.198844
108.155896	1631.485248	5.337178	-0.020319	2.204164
108.089971	1639.661633	5.342182	-0.020312	2.209504
108.471179	1647.738643	5.347187	-0.020388	2.214807
108.735532	1655.822761	5.352192	-0.020443	2.220092
109.640635	1663.819533	5.357197	-0.020617	2.225366
110.126301	1671.910275	5.362202	-0.020712	2.230649
110.300592	1680.025450	5.367206	-0.020750	2.235908
110.442438	1688.144306	5.372211	-0.020782	2.241154
110.433132	1696.259525	5.377216	-0.020785	2.246371
111.123947	1704.294994	5.382221	-0.020919	2.251588
111.591914	1712.347107	5.387226	-0.021011	2.256783
112.202080	1720.398738	5.392230	-0.021130	2.261979
112.302878	1728.559073	5.397235	-0.021154	2.267187
112.721913	1736.648660	5.402240	-0.021237	2.272366
113.214825	1744.678716	5.407245	-0.021334	2.277502
113.708646	1752.717006	5.412250	-0.021432	2.282631
114.216513	1760.755946	5.417254	-0.021531	2.287751
114.429169	1768.898094	5.422259	-0.021576	2.292898
114.645224	1776.978909	5.427264	-0.021622	2.297995
115.162953	1785.021931	5.432269	-0.021723	2.303083
115.343777	1793.130860	5.437274	-0.021762	2.308173
115.822240	1801.174503	5.442278	-0.021856	2.313235
116.388901	1809.230749	5.447283	-0.021967	2.318302
117.145663	1817.208506	5.452288	-0.022113	2.323326
117.527073	1825.302940	5.457293	-0.022189	2.328378
117.760879	1833.439247	5.462298	-0.022238	2.333433
118.037705	1841.533583	5.467302	-0.022295	2.338455
119.056470	1849.502049	5.472307	-0.022490	2.343451
119.523889	1857.579718	5.477312	-0.022582	2.348457
119.422954	1865.799760	5.482317	-0.022569	2.353492
119.430691	1873.895966	5.487322	-0.022575	2.358449
119.877724	1881.910925	5.492326	-0.022664	2.363383
120.402343	1889.965229	5.497331	-0.022767	2.368337
120.429760	1898.061990	5.502336	-0.022777	2.373265
120.638265	1906.179429	5.507341	-0.022821	2.378210
121.181396	1914.163749	5.512346	-0.022927	2.383092
121.754574	1922.182732	5.517350	-0.023039	2.387987
121.961075	1930.326474	5.522355	-0.023083	2.392918
122.527967	1938.314652	5.527360	-0.023194	2.397774
122.981441	1946.390809	5.532365	-0.023283	2.402663
123.038622	1954.516542	5.537370	-0.023299	2.407540
123.525225	1962.550917	5.542374	-0.023395	2.412388
123.777605	1970.648271	5.547379	-0.023447	2.417244
124.024728	1978.712718	5.552384	-0.023499	2.422070
124.391219	1986.805095	5.557389	-0.023572	2.426913
125.007166	1994.831202	5.562394	-0.023692	2.431727
125.118200	2002.941525	5.567398	-0.023718	2.436541
125.259982	2011.023990	5.572403	-0.023749	2.441331
125.784915	2019.005732	5.577408	-0.023852	2.446083
126.939726	2026.948386	5.582413	-0.024073	2.450851
126.859218	2035.120189	5.587418	-0.024063	2.455648
126.579524	2043.284405	5.592422	-0.024016	2.460417
127.191562	2051.293452	5.597427	-0.024135	2.465154
127.532322	2059.364419	5.602432	-0.024204	2.469897
127.738902	2067.451878	5.607437	-0.024248	2.474630
127.875252	2075.507278	5.612442	-0.024278	2.479330
128.185492	2083.518185	5.617446	-0.024341	2.484009
128.474776	2091.606679	5.622451	-0.024400	2.488722
128.762550	2099.632895	5.627456	-0.024459	2.493390
128.945127	2107.732948	5.632461	-0.024498	2.498084
128.902558	2115.825109	5.637466	-0.024495	2.502747
129.456845	2123.852060	5.642470	-0.024604	2.507410
129.908734	2131.905424	5.647475	-0.024693	2.512070
130.221638	2139.944918	5.652480	-0.024757	2.516704
130.626424	2147.982907	5.657485	-0.024837	2.521335
131.096785	2156.002038	5.662490	-0.024930	2.525952
131.425850	2164.083683	5.667494	-0.024997	2.530585
131.808261	2172.167175	5.672499	-0.025073	2.535215
131.817120	2180.262863	5.677504	-0.025080	2.539816
132.505868	2188.263910	5.682509	-0.025213	2.544404
133.007681	2196.312912	5.687514	-0.025312	2.548998
133.207234	2204.379508	5.692518	-0.025354	2.553571
133.528704	2212.460349	5.697523	-0.025419	2.558153
134.167310	2220.412480	5.702528	-0.025543	2.562677
134.419960	2228.503568	5.707533	-0.025596	2.567243
134.676732	2236.588376	5.712538	-0.025649	2.571798
134.933492	2244.661747	5.717542	-0.025702	2.576339
135.044969	2252.783601	5.722547	-0.025728	2.580888
135.770058	2260.731308	5.727552	-0.025868	2.585375
136.590006	2268.777742	5.732557	-0.026026	2.589916
137.529964	2276.848103	5.737562	-0.026206	2.594470
137.765656	2284.866386	5.742566	-0.026255	2.598939
138.390221	2292.900420	5.747571	-0.026377	2.603435
138.275878	2301.042145	5.752576	-0.026361	2.607931
138.310340	2309.158261	5.757581	-0.026372	2.612417
138.867075	2317.136793	5.762586	-0.026481	2.616854
139.484204	2325.139825	5.767590	-0.026601	2.621302
139.645286	2333.239652	5.772595	-0.026636	2.625764
140.078557	2341.264459	5.777600	-0.026722	2.630195
140.437703	2349.318289	5.782605	-0.026794	2.634630
140.778418	2357.372201	5.787610	-0.026863	2.639056
140.964007	2365.423888	5.792614	-0.026903	2.643463
141.205957	2373.507095	5.797619	-0.026953	2.647884
141.597085	2381.536398	5.802624	-0.027031	2.652278
142.260592	2389.555974	5.807629	-0.027160	2.656677
142.237224	2397.656079	5.812634	-0.027161	2.661067
142.613659	2405.695510	5.817638	-0.027236	2.665444
142.609797	2413.847751	5.822643	-0.027241	2.669849
142.879320	2421.860019	5.827648	-0.027296	2.674189
142.584612	2429.983610	5.832653	-0.027246	2.678545
142.861527	2437.991063	5.837658	-0.027303	2.682869
142.647687	2446.094243	5.842662	-0.027268	2.687205
143.161812	2454.113464	5.847667	-0.027369	2.691537
143.585404	2462.115479	5.852672	-0.027453	2.695846
143.781390	2470.168164	5.857677	-0.027495	2.700161
144.052466	2478.159719	5.862682	-0.027551	2.704441
144.271075	2486.238515	5.867686	-0.027597	2.708758
145.182197	2494.190151	5.872691	-0.027771	2.713044
145.368483	2502.218896	5.877696	-0.027811	2.717318
145.623894	2510.303350	5.882701	-0.027864	2.721620
145.820192	2518.383068	5.887706	-0.027906	2.725908
146.521590	2526.374123	5.892710	-0.028042	2.730174
146.248511	2534.568462	5.897715	-0.027996	2.734479
146.315274	2542.602563	5.902720	-0.028014	2.738715
147.093463	2550.543864	5.907725	-0.028164	2.742940
147.213802	2558.641275	5.912730	-0.028191	2.747199
147.114566	2566.789424	5.917734	-0.028178	2.751464
147.711489	2574.798076	5.922739	-0.028295	2.755693
147.549345	2582.846795	5.927744	-0.028270	2.759890
147.950428	2590.827697	5.932749	-0.028349	2.764079
148.372294	2598.843668	5.937754	-0.028433	2.768282
148.502857	2606.924526	5.942758	-0.028463	2.772494
148.795121	2614.981227	5.947763	-0.028522	2.776696
148.892347	2623.028110	5.952768	-0.028546	2.780876
149.502822	2631.015923	5.957773	-0.028664	2.785050
149.749878	2639.043650	5.962778	-0.028716	2.789216
150.067611	2647.099445	5.967782	-0.028780	2.793394
150.743338	2655.100736	5.972787	-0.028911	2.797560
150.608279	2663.225481	5.977792	-0.028891	2.801734
150.982471	2671.243292	5.982797	-0.028966	2.805877
151.019213	2679.347784	5.987802	-0.028978	2.810039
151.341109	2687.385439	5.992806	-0.029043	2.814177
151.655068	2695.445193	5.997811	-0.029107	2.818320
151.752769	2703.465008	6.002816	-0.029130	2.822424
152.397466	2711.469403	6.007821	-0.029255	2.826546
152.921216	2719.504727	6.012826	-0.029358	2.830670
153.662449	2727.465581	6.017830	-0.029501	2.834763
153.937389	2735.543083	6.022835	-0.029558	2.838883
154.351417	2743.549357	6.027840	-0.029640	2.842968
154.350281	2751.682243	6.032845	-0.029645	2.847087
155.035072	2759.657561	6.037850	-0.029778	2.851160
155.535654	2767.702847	6.042854	-0.029876	2.855252
155.706281	2775.774074	6.047859	-0.029913	2.859332
156.061944	2783.793664	6.052864	-0.029985	2.863391
156.505692	2791.848990	6.057869	-0.030072	2.867467
156.756667	2799.943517	6.062874	-0.030124	2.871546
156.905133	2807.976582	6.067878	-0.030157	2.875583
157.185503	2816.052271	6.072883	-0.030215	2.879642
157.343400	2824.081496	6.077888	-0.030249	2.883666
157.419341	2832.139404	6.082893	-0.030269	2.887694
157.843909	2840.165611	6.087898	-0.030353	2.891719
158.054009	2848.216675	6.092902	-0.030397	2.895740
158.307310	2856.271692	6.097907	-0.030450	2.899759
158.657868	2864.256670	6.102912	-0.030520	2.903743
158.755452	2872.354808	6.107917	-0.030543	2.907764
158.900386	2880.434956	6.112922	-0.030576	2.911773
159.157544	2888.462019	6.117926	-0.030629	2.915757
159.614541	2896.467230	6.122931	-0.030719	2.919735
159.719940	2904.469421	6.127936	-0.030744	2.923686
159.833645	2912.508863	6.132941	-0.030770	2.927652
159.973174	2920.565310	6.137946	-0.030801	2.931621
160.529082	2928.559433	6.142950	-0.030910	2.935578
160.700940	2936.608250	6.147955	-0.030947	2.939534
160.545882	2944.675915	6.152960	-0.030924	2.943477
160.870766	2952.739295	6.157965	-0.030989	2.947439
161.349113	2960.745077	6.162970	-0.031083	2.951375
161.397154	2968.821069	6.167974	-0.031098	2.955317
161.890548	2976.786763	6.172979	-0.031195	2.959224
162.341585	2984.769157	6.177984	-0.031284	2.963132
162.404163	2992.883707	6.182989	-0.031301	2.967078
162.955402	3000.875525	6.187994	-0.031409	2.970985
163.229664	3008.899823	6.192998	-0.031465	2.974887
163.428966	3017.015876	6.198003	-0.031507	2.978825
163.567098	3025.052432	6.203008	-0.031538	2.982717
164.189265	3033.030521	6.208013	-0.031659	2.986600
164.030863	3041.174023	6.213018	-0.031635	2.990517
164.356927	3049.158595	6.218022	-0.031701	2.994378
164.604333	3057.202377	6.223027	-0.031752	2.998258
164.852977	3065.214293	6.228032	-0.031803	3.002117
165.437134	3073.213822	6.233037	-0.031917	3.005983
165.378918	3081.337517	6.238042	-0.031912	3.009871
165.734916	3089.340052	6.243046	-0.031983	3.013717
166.913967	3097.251116	6.248051	-0.032208	3.017555
166.441894	3105.427981	6.253056	-0.032125	3.021432
166.354875	3113.521212	6.258061	-0.032114	3.025284
167.018342	3121.473813	6.263066	-0.032243	3.029102
166.872705	3129.593180	6.268070	-0.032221	3.032953
167.023230	3137.644212	6.273075	-0.032254	3.036782
167.258321	3145.624766	6.278080	-0.032303	3.040576
167.910656	3153.557775	6.283085	-0.032430	3.044365
167.954855	3161.642674	6.288090	-0.032443	3.048190
168.088541	3169.699295	6.293094	-0.032474	3.052001
168.635605	3177.750081	6.298099	-0.032581	3.055825
168.480560	3185.814083	6.303104	-0.032557	3.059616
168.808605	3193.835130	6.308109	-0.032623	3.063406
168.967470	3201.891157	6.313114	-0.032658	3.067199
169.197838	3209.945181	6.318118	-0.032706	3.070990
169.063480	3218.064319	6.323123	-0.032686	3.074790
169.535386	3225.978735	6.328128	-0.032779	3.078518
169.973958	3233.971232	6.333133	-0.032866	3.082276
169.714509	3242.080927	6.338138	-0.032823	3.086051
170.307569	3250.021867	6.343142	-0.032939	3.089783
170.325957	3258.130816	6.348147	-0.032947	3.093562
170.641749	3266.101135	6.353152	-0.033011	3.097285
170.886992	3274.160334	6.358157	-0.033062	3.101042
171.167211	3282.174058	6.363162	-0.033119	3.104775
171.481761	3290.196109	6.368166	-0.033183	3.108509
171.850593	3298.259573	6.373171	-0.033257	3.112260
172.294325	3306.278097	6.378176	-0.033345	3.115989
172.743017	3314.264708	6.383181	-0.033434	3.119700
173.009826	3322.303780	6.388186	-0.033489	3.123421
173.575753	3330.302139	6.393190	-0.033599	3.127133
173.607100	3338.443409	6.398195	-0.033610	3.130882
173.573374	3346.505172	6.403200	-0.033609	3.134586
173.911521	3354.510676	6.408205	-0.033677	3.138278
174.531638	3362.505797	6.413210	-0.033798	3.141973
174.576023	3370.552354	6.418214	-0.033811	3.145661
174.676337	3378.637641	6.423219	-0.033835	3.149365
174.972234	3386.648148	6.428224	-0.033896	3.153039
175.123793	3394.714622	6.433229	-0.033929	3.156728
175.046919	3402.753600	6.438234	-0.033920	3.160390
175.249898	3410.724861	6.443238	-0.033963	3.164029
175.466540	3418.837974	6.448243	-0.034008	3.167729
175.713300	3426.804409	6.453248	-0.034060	3.171360
175.642536	3434.882844	6.458253	-0.034052	3.175023
176.158871	3442.862094	6.463258	-0.034153	3.178663
175.958071	3450.948438	6.468262	-0.034121	3.182315
176.438699	3458.923639	6.473267	-0.034215	3.185943
177.278362	3466.853869	6.478272	-0.034377	3.189563
177.582815	3474.934833	6.483277	-0.034439	3.193222
177.348077	3483.065718	6.488282	-0.034400	3.196877
177.594886	3491.070387	6.493286	-0.034451	3.200491
178.122052	3499.023819	6.498291	-0.034555	3.204090
178.106249	3507.114592	6.503296	-0.034557	3.207724
178.384815	3515.155593	6.508301	-0.034614	3.211343
178.775192	3523.193688	6.513306	-0.034692	3.214962
178.843822	3531.236966	6.518310	-0.034710	3.218566
179.055826	3539.267911	6.523315	-0.034755	3.222166
179.132848	3547.286554	6.528320	-0.034774	3.225751
179.817705	3555.254199	6.533325	-0.034907	3.229334
180.430977	3563.251161	6.538330	-0.035026	3.232924
180.299313	3571.393908	6.543334	-0.035007	3.236543
180.780997	3579.366848	6.548339	-0.035102	3.240108
181.054771	3587.376883	6.553344	-0.035158	3.243677
181.317279	3595.394831	6.558349	-0.035212	3.247246
182.071650	3603.389587	6.563354	-0.035358	3.250820
182.144555	3611.465223	6.568358	-0.035376	3.254398
182.546468	3619.519690	6.573363	-0.035456	3.257976
182.463828	3627.581815	6.578368	-0.035446	3.261533
183.065479	3635.542178	6.583373	-0.035563	3.265070
182.655456	3643.715464	6.588378	-0.035492	3.268656
182.671271	3651.735949	6.593382	-0.035501	3.272187
182.858273	3659.788319	6.598387	-0.035541	3.275736
183.396275	3667.669873	6.603392	-0.035646	3.279220
183.512183	3675.738543	6.608397	-0.035673	3.282766
184.144142	3683.722167	6.613402	-0.035795	3.286291
184.498810	3691.752995	6.618406	-0.035867	3.289821
184.188577	3699.933576	6.623411	-0.035814	3.293387
184.434119	3707.911172	6.628416	-0.035865	3.296882
185.348639	3715.857761	6.633421	-0.036041	3.300387
185.590080	3723.898922	6.638426	-0.036091	3.303902
185.871136	3731.920785	6.643430	-0.036148	3.307407
186.368070	3739.982699	6.648435	-0.036246	3.310934
186.739431	3747.997259	6.653440	-0.036320	3.314432
187.122936	3755.996350	6.658445	-0.036397	3.317919
187.188964	3764.094606	6.663450	-0.036414	3.321434
187.137794	3772.113951	6.668454	-0.036410	3.324906
187.665162	3780.148219	6.673459	-0.036513	3.328403
187.631345	3788.183636	6.678464	-0.036512	3.331875
187.814854	3796.234775	6.683469	-0.036552	3.335359
188.196447	3804.222462	6.688474	-0.036628	3.338820
188.448868	3812.225767	6.693478	-0.036680	3.342278
188.708458	3820.291274	6.698483	-0.036734	3.345760
188.419582	3828.399358	6.703488	-0.036685	3.349236
188.637837	3836.396029	6.708493	-0.036731	3.352679
189.036166	3844.414999	6.713498	-0.036810	3.356136
189.652267	3852.330012	6.718502	-0.036930	3.359552
190.048693	3860.349979	6.723507	-0.037009	3.363002
190.095769	3868.421387	6.728512	-0.037023	3.366456
190.106092	3876.510174	6.733517	-0.037030	3.369914
190.582546	3884.543958	6.738522	-0.037124	3.373361
190.166901	3892.624255	6.743526	-0.037052	3.376792
191.044241	3900.553425	6.748531	-0.037221	3.380203
191.041865	3908.569419	6.753536	-0.037225	3.383615
191.034217	3916.687997	6.758541	-0.037229	3.387066
191.309850	3924.694838	6.763546	-0.037286	3.390477
191.489026	3932.729956	6.768550	-0.037324	3.393894
191.714437	3940.785504	6.773555	-0.037371	3.397316
191.840079	3948.786287	6.778560	-0.037400	3.400709
191.538729	3956.835300	6.783565	-0.037349	3.404103
191.686134	3964.894605	6.788570	-0.037382	3.407515
191.770344	3972.925269	6.793574	-0.037403	3.410908
192.141230	3980.910769	6.798579	-0.037477	3.414290
192.578191	3988.850590	6.803584	-0.037563	3.417651
193.073978	3996.877321	6.808589	-0.037661	3.421047
193.141614	4004.923840	6.813594	-0.037679	3.424434
193.185283	4012.987812	6.818598	-0.037692	3.427823
194.086648	4020.987850	6.823603	-0.037865	3.431212
193.915307	4029.018205	6.828608	-0.037838	3.434573
193.908723	4037.079882	6.833613	-0.037842	3.437949
194.489914	4045.073658	6.838618	-0.037956	3.441315
194.434195	4053.090358	6.843622	-0.037950	3.444664
194.317913	4061.172218	6.848627	-0.037934	3.448035
194.738736	4069.183076	6.853632	-0.038017	3.451392
195.575367	4077.092688	6.858637	-0.038178	3.454717
195.335572	4085.230955	6.863642	-0.038139	3.458098
195.586830	4093.248149	6.868646	-0.038191	3.461441
195.818063	4101.313192	6.873651	-0.038239	3.464801
195.615170	4109.316337	6.878656	-0.038207	3.468117
196.112718	4117.318886	6.883661	-0.038304	3.471453
196.273369	4125.380899	6.888666	-0.038340	3.474799
196.778679	4133.306602	6.893670	-0.038439	3.478097
196.789310	4141.427388	6.898675	-0.038446	3.481456
196.989137	4149.381997	6.903680	-0.038488	3.484750
197.227193	4157.413791	6.908685	-0.038538	3.488073
197.358637	4165.523282	6.913690	-0.038568	3.491422
197.470204	4173.514855	6.918694	-0.038594	3.494718
198.107592	4181.485634	6.923699	-0.038717	3.498020
197.976560	4189.597717	6.928704	-0.038698	3.501351
198.085750	4197.572143	6.933709	-0.038724	3.504631
198.747596	4205.598494	6.938714	-0.038852	3.507947
198.977136	4213.596914	6.943718	-0.038900	3.511234
199.099004	4221.669397	6.948723	-0.038928	3.514545
199.254487	4229.681272	6.953728	-0.038962	3.517829
199.644413	4237.747213	6.958733	-0.039040	3.521139
200.027255	4245.670094	6.963738	-0.039116	3.524388
199.903993	4253.762513	6.968742	-0.039099	3.527687
200.253080	4261.830960	6.973747	-0.039169	3.530988
200.452680	4269.820614	6.978752	-0.039211	3.534249
200.811507	4277.834549	6.983757	-0.039283	3.537522
201.025690	4285.901848	6.988762	-0.039328	3.540808
201.264881	4293.826417	6.993766	-0.039378	3.544035
201.412007	4301.961672	6.998771	-0.039411	3.547341
201.701907	4309.960349	7.003776	-0.039470	3.550593
202.150003	4318.008345	7.008781	-0.039558	3.553867
201.948425	4326.103624	7.013786	-0.039526	3.557137
201.916720	4334.063533	7.018790	-0.039525	3.560355
202.289064	4342.047831	7.023795	-0.039600	3.563592
202.523363	4350.033789	7.028800	-0.039649	3.566822
202.543586	4358.097527	7.033805	-0.039658	3.570074
202.979223	4366.116338	7.038810	-0.039744	3.573318
203.334497	4374.116100	7.043814	-0.039815	3.576549
203.638732	4382.124769	7.048819	-0.039877	3.579779
204.142252	4390.094013	7.053824	-0.039976	3.582995
204.076597	4398.198778	7.058829	-0.039969	3.586247
204.146588	4406.242353	7.063834	-0.039987	3.589475
204.416293	4414.254977	7.068838	-0.040043	3.592693
204.635930	4422.358213	7.073843	-0.040089	3.595943
204.914647	4430.262253	7.078848	-0.040146	3.599113
205.092771	4438.328542	7.083853	-0.040184	3.602341
205.033187	4446.386780	7.088858	-0.040178	3.605557
205.035497	4454.399884	7.093862	-0.040184	3.608753
205.960132	4462.349488	7.098867	-0.040361	3.611948
206.175244	4470.398336	7.103872	-0.040406	3.615159
205.983335	4478.530387	7.108877	-0.040376	3.618388
206.433585	4486.516929	7.113882	-0.040465	3.621576
206.369471	4494.507046	7.118886	-0.040458	3.624747
207.396462	4502.460802	7.123891	-0.040655	3.627932
207.489842	4510.543598	7.128896	-0.040677	3.631138
207.382879	4518.586458	7.133901	-0.040662	3.634321
208.141887	4526.566430	7.138906	-0.040809	3.637500
208.094239	4534.661103	7.143910	-0.040805	3.640698
207.560647	4542.731063	7.148915	-0.040711	3.643871
207.669882	4550.737639	7.153920	-0.040737	3.647034
208.484110	4558.655351	7.158925	-0.040893	3.650179
208.553918	4566.706569	7.163930	-0.040912	3.653353
208.647198	4574.754446	7.168934	-0.040934	3.656523
208.825422	4582.788301	7.173939	-0.040973	3.659687
208.840730	4590.808018	7.178944	-0.040981	3.662839
208.499461	4598.933549	7.183949	-0.040922	3.666020
208.730305	4606.933776	7.188954	-0.040970	3.669164
208.867679	4614.917186	7.193958	-0.041001	3.672297
209.368456	4622.899059	7.198963	-0.041100	3.675436
209.155173	4630.962854	7.203968	-0.041065	3.678585
209.673239	4638.952736	7.208973	-0.041167	3.681723
209.962497	4646.936599	7.213978	-0.041226	3.684849
210.341747	4654.905207	7.218982	-0.041302	3.687968
210.332883	4663.068255	7.223987	-0.041305	3.691151
210.524051	4671.060374	7.228992	-0.041346	3.694270
210.494243	4679.110451	7.233997	-0.041346	3.697402
211.002476	4687.125298	7.239002	-0.041445	3.700533
211.162833	4695.103134	7.244006	-0.041480	3.703637
211.249583	4703.153031	7.249011	-0.041502	3.706764
211.544342	4711.144281	7.254016	-0.041562	3.709872
211.535912	4719.261779	7.259021	-0.041566	3.713018
211.852287	4727.286258	7.264026	-0.041630	3.716134
212.022381	4735.173180	7.269030	-0.041666	3.719190
212.223050	4743.280340	7.274035	-0.041709	3.722329
212.753884	4751.226255	7.279040	-0.041813	3.725412
212.869445	4759.263028	7.284045	-0.041840	3.728517
213.119760	4767.325234	7.289050	-0.041892	3.731633
213.356365	4775.303600	7.294054	-0.041941	3.734713
213.691337	4783.359303	7.299059	-0.042008	3.737823
213.491317	4791.421012	7.304064	-0.041976	3.740919
213.504635	4799.429137	7.309069	-0.041984	3.743997
214.087353	4807.446829	7.314074	-0.042098	3.747091
214.304464	4815.444560	7.319078	-0.042143	3.750165
214.199768	4823.539738	7.324083	-0.042129	3.753266
214.372103	4831.542256	7.329088	-0.042166	3.756336
214.807155	4839.466047	7.334093	-0.042252	3.759380
214.999476	4847.525459	7.339098	-0.042293	3.762467
215.094269	4855.526680	7.344102	-0.042316	3.765526
215.557902	4863.559327	7.349107	-0.042408	3.768605
215.342667	4871.653136	7.354112	-0.042373	3.771687
215.841913	4879.597016	7.359117	-0.042471	3.774728
216.038573	4887.670680	7.364122	-0.042513	3.777807
216.097076	4895.680896	7.369126	-0.042529	3.780857
216.205597	4903.704346	7.374131	-0.042554	3.783911
216.832705	4911.681498	7.379136	-0.042676	3.786957
216.883348	4919.762829	7.384141	-0.042691	3.790026
217.039172	4927.812124	7.389146	-0.042725	3.793083
217.326668	4935.786532	7.394150	-0.042784	3.796112
217.787731	4943.760071	7.399155	-0.042875	3.799143
218.114913	4951.792133	7.404160	-0.042941	3.802190
217.876127	4959.848011	7.409165	-0.042902	3.805231
218.195215	4967.894456	7.414170	-0.042966	3.808278
218.900984	4975.830537	7.419174	-0.043103	3.811290
219.060318	4983.879959	7.424179	-0.043138	3.814330
219.288275	4991.937542	7.429184	-0.043185	3.817372
219.344912	4999.975467	7.434189	-0.043201	3.820400
219.312511	5007.999405	7.439194	-0.043200	3.823419
219.512323	5016.018303	7.444198	-0.043243	3.826439
220.051623	5024.056676	7.449203	-0.043348	3.829471
220.234704	5032.057901	7.454208	-0.043388	3.832478
220.618267	5040.047816	7.459213	-0.043464	3.835484
220.806209	5048.104865	7.464218	-0.043504	3.838508
221.031932	5056.116100	7.469222	-0.043552	3.841513
221.212606	5064.101297	7.474227	-0.043590	3.844505
221.564300	5072.154655	7.479232	-0.043661	3.847524
222.140325	5080.134579	7.484237	-0.043773	3.850518
222.146289	5088.252729	7.489242	-0.043780	3.853549
221.736771	5096.311693	7.494246	-0.043709	3.856547
222.273561	5104.288763	7.499251	-0.043814	3.859532
222.615599	5112.271682	7.504256	-0.043883	3.862512
222.768819	5120.323750	7.509261	-0.043916	3.865512
222.981248	5128.323342	7.514266	-0.043961	3.868491
223.741043	5136.306522	7.519270	-0.044108	3.871474
223.628881	5144.521346	7.524275	-0.044092	3.874521
223.693897	5152.481737	7.529280	-0.044110	3.877476
224.114956	5160.387784	7.534285	-0.044193	3.880416
224.417354	5168.356405	7.539290	-0.044255	3.883374
224.653026	5176.399090	7.544294	-0.044304	3.886356
225.114234	5184.361208	7.549299	-0.044395	3.889310
225.598175	5192.460160	7.554304	-0.044490	3.892313
225.134754	5200.552779	7.559309	-0.044409	3.895292
225.044208	5208.609721	7.564314	-0.044397	3.898263
225.215593	5216.599123	7.569318	-0.044434	3.901213
225.397564	5224.588140	7.574323	-0.044473	3.904160
225.649920	5232.602350	7.579328	-0.044526	3.907116
226.163717	5240.569508	7.584333	-0.044626	3.910057
226.229466	5248.627437	7.589338	-0.044644	3.913020
225.995200	5256.645600	7.594342	-0.044605	3.915961
226.394266	5264.652724	7.599347	-0.044685	3.918908
226.473590	5272.701886	7.604352	-0.044705	3.921861
226.877236	5280.650397	7.609357	-0.044785	3.924782
227.295161	5288.710855	7.614362	-0.044868	3.927742
227.648137	5296.667503	7.619366	-0.044939	3.930661
227.626142	5304.802016	7.624371	-0.044940	3.933635
227.680094	5312.817318	7.629376	-0.044955	3.936564
227.749344	5320.825845	7.634381	-0.044974	3.939490
228.100902	5328.850475	7.639386	-0.045044	3.942424
228.314679	5336.824144	7.644390	-0.045089	3.945335
228.244423	5344.952233	7.649395	-0.045081	3.948295
228.633299	5352.906590	7.654400	-0.045159	3.951198
228.815639	5360.894744	7.659405	-0.045198	3.954107
229.123013	5368.976129	7.664410	-0.045260	3.957050
229.449075	5376.919976	7.669414	-0.045326	3.959941
229.419943	5384.990201	7.674419	-0.045326	3.962869
229.665548	5392.994804	7.679424	-0.045377	3.965777
229.983277	5400.999177	7.684429	-0.045441	3.968684
229.968100	5409.116814	7.689434	-0.045444	3.971623
230.002843	5417.096428	7.694438	-0.045455	3.974511
230.314222	5425.156197	7.699443	-0.045519	3.977431
230.324463	5433.160032	7.704448	-0.045526	3.980323
230.619414	5441.077792	7.709453	-0.045586	3.983187
230.981853	5449.167721	7.714458	-0.045658	3.986113
231.021674	5457.163485	7.719462	-0.045671	3.988996
231.118793	5465.233345	7.724467	-0.045694	3.991905
231.305776	5473.190262	7.729472	-0.045734	3.994773
232.006892	5481.164555	7.734477	-0.045870	3.997654
231.953078	5489.250806	7.739482	-0.045865	4.000560
231.836799	5497.249416	7.744486	-0.045849	4.003431
232.044138	5505.340913	7.749491	-0.045893	4.006340
232.250648	5513.294764	7.754496	-0.045936	4.009196
232.442500	5521.350049	7.759501	-0.045977	4.012087
232.876623	5529.333520	7.764506	-0.046063	4.014954
232.967826	5537.372178	7.769510	-0.046085	4.017833
233.110753	5545.393267	7.774515	-0.046117	4.020704
233.461125	5553.352808	7.779520	-0.046187	4.023555
233.771530	5561.383839	7.784525	-0.046250	4.026428
233.899326	5569.431820	7.789530	-0.046279	4.029303
233.981148	5577.523630	7.794534	-0.046300	4.032190
234.783775	5585.507594	7.799539	-0.046455	4.035048
234.841763	5593.514918	7.804544	-0.046470	4.037901
235.173863	5601.492650	7.809549	-0.046537	4.040745
235.214577	5609.555213	7.814554	-0.046550	4.043613
235.795920	5617.498078	7.819558	-0.046664	4.046445
236.066205	5625.531963	7.824563	-0.046719	4.049302
236.095211	5633.578908	7.829568	-0.046730	4.052158
236.078482	5641.645915	7.834573	-0.046732	4.055019
236.647842	5649.614209	7.839578	-0.046843	4.057851
236.852417	5657.604409	7.844582	-0.046886	4.060684
237.073795	5665.644556	7.849587	-0.046933	4.063533
237.201812	5673.704243	7.854592	-0.046962	4.066384
237.549040	5681.678793	7.859597	-0.047032	4.069208
237.653303	5689.781005	7.864602	-0.047056	4.072070
238.175785	5697.699222	7.869606	-0.047159	4.074872
238.145066	5705.766441	7.874611	-0.047158	4.077716
238.555382	5713.747754	7.879616	-0.047240	4.080535
238.662746	5721.772491	7.884621	-0.047265	4.083362
239.025261	5729.863038	7.889626	-0.047338	4.086215
239.241847	5737.819889	7.894630	-0.047383	4.089016
239.505881	5745.895846	7.899635	-0.047437	4.091857
239.523725	5753.890873	7.904640	-0.047446	4.094665
239.794241	5761.948538	7.909645	-0.047502	4.097496
239.966953	5769.985662	7.914650	-0.047539	4.100317
239.896105	5777.960893	7.919654	-0.047531	4.103110
240.397085	5785.967146	7.924659	-0.047629	4.105921
241.342080	5793.874413	7.929664	-0.047810	4.108702
241.349646	5802.013951	7.934669	-0.047817	4.111548
241.550771	5810.002062	7.939674	-0.047860	4.114342
241.978896	5817.999982	7.944678	-0.047945	4.117141
241.771165	5826.094309	7.949683	-0.047911	4.119963
242.502507	5834.033117	7.954688	-0.048052	4.122741
242.640855	5842.060241	7.959693	-0.048083	4.125541
243.319933	5850.073354	7.964698	-0.048215	4.128340
243.031141	5858.213633	7.969702	-0.048167	4.131169
243.333099	5866.195322	7.974707	-0.048228	4.133949
243.110498	5874.264002	7.979712	-0.048192	4.136750
243.821562	5882.113132	7.984717	-0.048329	4.139486
244.002180	5890.196923	7.989722	-0.048368	4.142293
243.906384	5898.226621	7.994726	-0.048355	4.145077
243.957614	5906.301141	7.999731	-0.048370	4.147876
244.643357	5914.281372	8.004736	-0.048503	4.150649
245.023290	5922.260706	8.009741	-0.048579	4.153416
244.882003	5930.353548	8.014746	-0.048558	4.156213
244.636949	5938.332780	8.019750	-0.048517	4.158968
244.979530	5946.384920	8.024755	-0.048586	4.161754
245.082737	5954.347392	8.029760	-0.048611	4.164504
245.346783	5962.359971	8.034765	-0.048665	4.167271
245.619052	5970.388565	8.039770	-0.048721	4.170042
245.420457	5978.432466	8.044774	-0.048689	4.172811
246.083871	5986.452313	8.049779	-0.048818	4.175580
245.915617	5994.480410	8.054784	-0.048792	4.178340
246.292183	6002.493378	8.059789	-0.048867	4.181099
246.463045	6010.452757	8.064794	-0.048904	4.183836
246.551820	6018.473991	8.069798	-0.048926	4.186591
247.141223	6026.479317	8.074803	-0.049041	4.189345
247.125313	6034.596931	8.079808	-0.049043	4.192128
247.180664	6042.631794	8.084813	-0.049058	4.194882
247.473043	6050.655567	8.089818	-0.049118	4.197633
247.769066	6058.611598	8.094822	-0.049178	4.200360
248.038106	6066.619508	8.099827	-0.049234	4.203101
248.269143	6074.602074	8.104832	-0.049282	4.205832
248.429439	6082.623409	8.109837	-0.049317	4.208574
248.550585	6090.730052	8.114842	-0.049345	4.211342
248.321791	6098.756718	8.119846	-0.049307	4.214077
248.572649	6106.787248	8.124851	-0.049359	4.216817
249.117582	6114.713476	8.129856	-0.049466	4.219523
249.376942	6122.725031	8.134861	-0.049519	4.222254
250.035058	6130.724292	8.139866	-0.049647	4.224982
250.390624	6138.689204	8.144870	-0.049718	4.227694
250.398184	6146.830538	8.149875	-0.049725	4.230460
250.608977	6154.863085	8.154880	-0.049769	4.233190
250.581164	6162.908504	8.159885	-0.049769	4.235919
250.895458	6170.831319	8.164890	-0.049833	4.238609
250.881074	6178.909718	8.169894	-0.049836	4.241347
250.909596	6186.877646	8.174899	-0.049846	4.244045
250.970347	6194.956706	8.179904	-0.049863	4.246780
251.405563	6202.904795	8.184909	-0.049949	4.249473
251.530390	6210.984972	8.189914	-0.049977	4.252205
251.757084	6218.943409	8.194918	-0.050025	4.254896
251.885982	6227.057969	8.199923	-0.050054	4.257636
251.974838	6235.033678	8.204928	-0.050076	4.260328
252.005904	6243.045844	8.209933	-0.050087	4.263029
252.393884	6251.084032	8.214938	-0.050164	4.265741
251.775426	6259.115446	8.219942	-0.050054	4.268439
252.500083	6267.085429	8.224947	-0.050194	4.271128
252.691551	6275.100402	8.229952	-0.050235	4.273825
252.650625	6283.127242	8.234957	-0.050232	4.276522
252.752076	6291.089960	8.239962	-0.050257	4.279198
253.181058	6299.112569	8.244966	-0.050342	4.281894
253.360542	6307.100933	8.249971	-0.050380	4.284576
253.186078	6315.241290	8.254976	-0.050353	4.287303
253.716683	6323.136806	8.259981	-0.050457	4.289953
253.726805	6331.249624	8.264986	-0.050464	4.292669
253.971068	6339.225797	8.269990	-0.050515	4.295340
254.383863	6347.284624	8.274995	-0.050597	4.298038
254.696294	6355.223376	8.280000	-0.050660	4.300694
254.552381	6363.228101	8.285005	-0.050638	4.303365
254.675784	6371.355988	8.290010	-0.050667	4.306079
254.874726	6379.309144	8.295014	-0.050709	4.308733
255.227619	6387.349430	8.300019	-0.050780	4.311416
255.373711	6395.312162	8.305024	-0.050812	4.314070
255.609621	6403.361959	8.310029	-0.050861	4.316752
255.677603	6411.388341	8.315034	-0.050879	4.319423
255.671659	6419.413166	8.320038	-0.050883	4.322091
256.305502	6427.348692	8.325043	-0.051006	4.324733
256.351632	6435.428289	8.330048	-0.051020	4.327416
256.633198	6443.397878	8.335053	-0.051078	4.330064
257.320357	6451.407598	8.340058	-0.051211	4.332726
257.351579	6459.472599	8.345062	-0.051222	4.335399
257.769161	6467.458681	8.350067	-0.051305	4.338048
257.970636	6475.504111	8.355072	-0.051347	4.340713
258.138245	6483.449664	8.360077	-0.051384	4.343343
258.195028	6491.584104	8.365082	-0.051400	4.346033
258.138569	6499.535374	8.370086	-0.051394	4.348659
258.937873	6507.570668	8.375091	-0.051548	4.351319
259.266510	6515.594712	8.380096	-0.051615	4.353970
259.347689	6523.638013	8.385101	-0.051635	4.356623
259.540406	6531.610753	8.390106	-0.051676	4.359252
259.838509	6539.601171	8.395110	-0.051737	4.361887
259.707320	6547.623270	8.400115	-0.051717	4.364527
260.308781	6555.633858	8.405120	-0.051835	4.367167
260.580601	6563.596036	8.410125	-0.051890	4.369787
260.501219	6571.734259	8.415130	-0.051881	4.372460
260.853060	6579.708326	8.420134	-0.051952	4.375082
260.709615	6587.766481	8.425139	-0.051930	4.377725
261.521409	6595.698664	8.430144	-0.052086	4.380333
262.036544	6603.672654	8.435149	-0.052187	4.382950
262.222551	6611.795778	8.440154	-0.052227	4.385613
261.800835	6619.866878	8.445158	-0.052154	4.388252
261.924090	6627.917178	8.450163	-0.052182	4.390887
262.229553	6635.840698	8.455168	-0.052244	4.393480
262.568423	6643.875378	8.460173	-0.052312	4.396109
262.640071	6651.864882	8.465178	-0.052331	4.398719
262.502985	6659.955132	8.470182	-0.052311	4.401359
262.797507	6667.898163	8.475187	-0.052371	4.403952
263.268665	6675.944114	8.480192	-0.052464	4.406578
263.595117	6683.903908	8.485197	-0.052530	4.409174
263.892597	6691.997587	8.490202	-0.052590	4.411811
264.074732	6699.962139	8.495206	-0.052629	4.414404
264.284623	6708.065362	8.500211	-0.052674	4.417041
264.077060	6716.066861	8.505216	-0.052640	4.419641
264.825162	6724.045048	8.510221	-0.052785	4.422237
265.373155	6732.017401	8.515226	-0.052892	4.424829
265.268689	6740.159291	8.520230	-0.052878	4.427470
265.643288	6748.157941	8.525235	-0.052952	4.430066
265.590827	6756.276794	8.530240	-0.052948	4.432697
266.061592	6764.188015	8.535245	-0.053041	4.435262
266.312139	6772.247643	8.540250	-0.053093	4.437872
266.601889	6780.229413	8.545254	-0.053152	4.440456
266.498007	6788.234086	8.550259	-0.053138	4.443043
266.590169	6796.268199	8.555264	-0.053160	4.445640
266.749072	6804.305971	8.560269	-0.053195	4.448236
267.181879	6812.320897	8.565274	-0.053280	4.450825
267.132274	6820.342501	8.570279	-0.053276	4.453413
267.171488	6828.429366	8.575283	-0.053289	4.456020
267.722877	6836.329883	8.580288	-0.053397	4.458568
267.902692	6844.365924	8.585293	-0.053435	4.461156
268.114784	6852.356734	8.590298	-0.053480	4.463729
268.495719	6860.364301	8.595303	-0.053556	4.466306
269.036054	6868.406377	8.600307	-0.053662	4.468894
269.059918	6876.462754	8.605312	-0.053672	4.471482
268.819077	6884.428380	8.610317	-0.053632	4.474038
268.894863	6892.560441	8.615322	-0.053651	4.476648
269.019791	6900.492100	8.620327	-0.053680	4.479192
269.365120	6908.522746	8.625331	-0.053749	4.481767
269.737033	6916.472976	8.630336	-0.053824	4.484315
270.084990	6924.501365	8.635341	-0.053894	4.486887
270.388656	6932.489210	8.640346	-0.053955	4.489444
270.755404	6940.522919	8.645351	-0.054029	4.492014
270.943515	6948.621310	8.650355	-0.054069	4.494603
271.093748	6956.598793	8.655360	-0.054102	4.497152
271.359817	6964.564765	8.660365	-0.054157	4.499695
271.699244	6972.649978	8.665370	-0.054225	4.502276
271.623998	6980.624446	8.670375	-0.054216	4.504818
271.622177	6988.698577	8.675379	-0.054221	4.507391
271.858900	6996.710837	8.680384	-0.054271	4.509944
272.436532	7004.643414	8.685389	-0.054383	4.512471
272.635294	7012.730192	8.690394	-0.054425	4.515044
272.325414	7020.780094	8.695399	-0.054373	4.517602
272.835539	7028.695884	8.700403	-0.054473	4.520119
272.878521	7036.701869	8.705408	-0.054486	4.522661
273.273292	7044.678232	8.710413	-0.054565	4.525194
273.301750	7052.754515	8.715418	-0.054575	4.527756
273.573530	7060.720665	8.720423	-0.054631	4.530283
273.852146	7068.762273	8.725427	-0.054688	4.532831
274.332549	7076.801659	8.730432	-0.054783	4.535379
274.541230	7084.794046	8.735437	-0.054827	4.537909
274.489971	7092.891117	8.740442	-0.054823	4.540470
274.849373	7100.808270	8.745447	-0.054895	4.542974
275.225431	7108.869159	8.750451	-0.054970	4.545521
275.677567	7116.841108	8.755456	-0.055059	4.548040
275.115060	7124.979583	8.760461	-0.054960	4.550607
275.797881	7132.933979	8.765466	-0.055092	4.553118
276.404963	7140.895631	8.770471	-0.055210	4.555629
276.759558	7148.883725	8.775475	-0.055281	4.558146
276.968980	7156.948899	8.780480	-0.055326	4.560687
277.087061	7164.928045	8.785485	-0.055353	4.563198
277.371759	7173.020643	8.790490	-0.055411	4.565744
277.552573	7180.958667	8.795495	-0.055450	4.568240
277.962479	7189.079452	8.800499	-0.055531	4.570792
277.960796	7197.054525	8.805504	-0.055536	4.573296
277.925127	7205.083952	8.810509	-0.055535	4.575816
278.521341	7213.044140	8.815514	-0.055651	4.578314
278.525638	7221.151981	8.820519	-0.055657	4.580855
278.428492	7229.118408	8.825523	-0.055644	4.583351
278.500828	7237.180932	8.830528	-0.055663	4.585876
279.365559	7245.085923	8.835533	-0.055829	4.588351
279.574139	7253.204676	8.840538	-0.055873	4.590891
279.965572	7261.109308	8.845543	-0.055951	4.593363
280.173696	7269.201168	8.850547	-0.055995	4.595891
279.895062	7277.245862	8.855552	-0.055948	4.598403
280.018587	7285.218992	8.860557	-0.055976	4.600891
280.578256	7293.186601	8.865562	-0.056086	4.603377
280.822566	7301.194102	8.870567	-0.056136	4.605874
280.616907	7309.257933	8.875571	-0.056103	4.608386
281.178073	7317.299161	8.880576	-0.056213	4.610891
281.029972	7325.295324	8.885581	-0.056191	4.613380
281.683869	7333.302107	8.890586	-0.056318	4.615871
281.291706	7341.327822	8.895591	-0.056250	4.618366
281.534783	7349.380980	8.900595	-0.056300	4.620868
281.571236	7357.380855	8.905600	-0.056312	4.623353
281.888072	7365.325982	8.910605	-0.056376	4.625819
282.316672	7373.382925	8.915610	-0.056461	4.628319
282.532403	7381.404576	8.920615	-0.056507	4.630806
283.319303	7389.330743	8.925619	-0.056658	4.633263
283.183930	7397.440534	8.930624	-0.056638	4.635775
283.547479	7405.370277	8.935629	-0.056711	4.638230
283.311468	7413.535345	8.940634	-0.056673	4.640756
283.247408	7421.465218	8.945639	-0.056666	4.643208
283.727320	7429.450251	8.950643	-0.056760	4.645676
284.251031	7437.474065	8.955648	-0.056863	4.648154
284.335917	7445.513770	8.960653	-0.056884	4.650636
284.270733	7453.570018	8.965658	-0.056877	4.653122
284.937964	7461.532168	8.970663	-0.057006	4.655577
284.965231	7469.581887	8.975667	-0.057017	4.658058
285.024887	7477.659238	8.980672	-0.057033	4.660547
285.158985	7485.590850	8.985677	-0.057063	4.662989
285.535213	7493.618148	8.990682	-0.057138	4.665459
285.506186	7501.621119	8.995687	-0.057138	4.667920
285.732106	7509.695601	9.000691	-0.057185	4.670402
285.691488	7517.746726	9.005696	-0.057183	4.672876
286.292479	7525.674827	9.010701	-0.057300	4.675310
286.332644	7533.751948	9.015706	-0.057313	4.677789
286.599885	7541.652551	9.020711	-0.057368	4.680212
286.973276	7549.674704	9.025715	-0.057442	4.682671
286.915581	7557.731907	9.030720	-0.057437	4.685140
287.059078	7565.755063	9.035725	-0.057469	4.687597
287.425270	7573.760605	9.040730	-0.057542	4.690047
287.658446	7581.745626	9.045735	-0.057591	4.692490
287.803074	7589.737712	9.050739	-0.057623	4.694934
288.067367	7597.851908	9.055744	-0.057677	4.697413
288.408021	7605.773432	9.060749	-0.057746	4.699832
288.800344	7613.805741	9.065754	-0.057824	4.702284
289.188270	7621.754368	9.070759	-0.057901	4.704709
288.994455	7629.922088	9.075763	-0.057871	4.707200
288.931027	7637.993167	9.080768	-0.057864	4.709660
289.245894	7645.947054	9.085773	-0.057928	4.712083
289.576355	7653.921642	9.090778	-0.057995	4.714510
289.704305	7661.940580	9.095783	-0.058024	4.716951
290.189458	7669.857657	9.100787	-0.058119	4.719358
290.568423	7677.971555	9.105792	-0.058195	4.721824
290.925780	7685.873904	9.110797	-0.058266	4.724225
290.825346	7694.076136	9.115802	-0.058253	4.726716
290.520478	7702.048993	9.120807	-0.058201	4.729136
291.380911	7710.036734	9.125811	-0.058367	4.731558
291.365120	7718.008180	9.130816	-0.058369	4.733975
291.573153	7726.110808	9.135821	-0.058413	4.736430
291.835318	7734.099513	9.140826	-0.058467	4.738849
291.914950	7742.128337	9.145831	-0.058487	4.741280
292.443364	7750.080777	9.150835	-0.058591	4.743685
292.858072	7758.147156	9.155840	-0.058673	4.746124
292.799177	7766.173118	9.160845	-0.058667	4.748550
293.211974	7774.201489	9.165850	-0.058749	4.750974
293.236098	7782.213597	9.170855	-0.058759	4.753393
293.775167	7790.175867	9.175859	-0.058865	4.755795
294.224021	7798.157186	9.180864	-0.058953	4.758202
294.404166	7806.173675	9.185869	-0.058992	4.760618
294.371049	7814.297199	9.190874	-0.058991	4.763066
294.465511	7822.250760	9.195879	-0.059014	4.765461
294.752035	7830.218348	9.200883	-0.059072	4.767859
294.917015	7838.331171	9.205888	-0.059108	4.770299
294.751270	7846.361079	9.210893	-0.059083	4.772715
294.893792	7854.340735	9.215898	-0.059114	4.775113
295.029855	7862.354549	9.220903	-0.059145	4.777520
295.476314	7870.383807	9.225907	-0.059233	4.779929
295.589372	7878.428553	9.230912	-0.059259	4.782343
295.391895	7886.370162	9.235917	-0.059228	4.784726
296.367408	7894.420469	9.240922	-0.059415	4.787136
297.049259	7902.382506	9.245927	-0.059547	4.789520
296.981493	7910.450230	9.250931	-0.059539	4.791936
297.065701	7918.451684	9.255936	-0.059560	4.794331
297.253389	7926.506340	9.260941	-0.059600	4.796741
297.801895	7934.421960	9.265946	-0.059708	4.799106
298.232440	7942.477216	9.270951	-0.059793	4.801512
298.363104	7950.439099	9.275955	-0.059822	4.803890
298.274980	7958.574952	9.280960	-0.059811	4.806319
298.488131	7966.510304	9.285965	-0.059856	4.808687
298.800999	7974.668638	9.290970	-0.059920	4.811119
299.064482	7982.542565	9.295975	-0.059974	4.813466
299.032408	7990.016382	9.300979	-0.059973	4.815693
299.175320	7994.733543	9.305984	-0.060002	4.817098

299.608898	7997.019191	9.310989	-0.060084	4.817777
299.552032	7998.559681	9.315994	-0.060075	4.818236
299.256084	7999.537292	9.320999	-0.060020	4.818528
299.509837	7999.569919	9.326003	-0.060068	4.818536
299.603571	7999.617261	9.331008	-0.060085	4.818550
300.076690	8000.283978	9.336013	-0.060173	4.818747
299.935646	7999.961279	9.341018	-0.060147	4.818651
300.051934	8000.084415	9.346023	-0.060169	4.818688
300.490689	8000.044984	9.351027	-0.060250	4.818674
300.334863	8000.046116	9.356032	-0.060221	4.818675
300.454924	7999.966919	9.361037	-0.060244	4.818651
300.917446	8000.180514	9.366042	-0.060330	4.818713
300.879517	8000.225113	9.371047	-0.060323	4.818726
300.936622	8000.131470	9.376051	-0.060333	4.818698
301.121314	8000.044718	9.381056	-0.060367	4.818672
300.963034	8000.073082	9.386061	-0.060338	4.818681
301.179675	8000.020298	9.391066	-0.060378	4.818664
301.163775	7999.916276	9.396071	-0.060375	4.818633
301.330089	8000.065229	9.401075	-0.060406	4.818677
301.318277	8000.185668	9.406080	-0.060404	4.818713
300.964565	7999.927329	9.411085	-0.060338	4.818637
300.874481	7999.798232	9.416090	-0.060321	4.818599
301.204934	7999.982857	9.421095	-0.060383	4.818653
301.820799	8000.075746	9.426099	-0.060497	4.818678
302.045646	8000.133178	9.431104	-0.060539	4.818694
302.163204	8000.058142	9.436109	-0.060561	4.818672
302.029128	8000.050115	9.441114	-0.060536	4.818670
302.006469	8000.058209	9.446119	-0.060532	4.818672
301.875057	7999.940109	9.451123	-0.060507	4.818638
301.970603	7999.941340	9.456128	-0.060525	4.818638
301.974753	8000.022137	9.461133	-0.060526	4.818662
301.761768	8000.073913	9.466138	-0.060486	4.818678
301.818853	7999.911058	9.471143	-0.060497	4.818629
301.851563	7999.968105	9.476147	-0.060503	4.818646
301.927288	7999.898820	9.481152	-0.060517	4.818625
301.351528	7999.944865	9.486157	-0.060409	4.818641
301.713037	7999.804817	9.491162	-0.060477	4.818598
301.570955	8000.010611	9.496167	-0.060450	4.818660
301.334102	7999.808310	9.501171	-0.060406	4.818600
301.352786	7999.815889	9.506176	-0.060409	4.818603
301.321300	7999.890981	9.511181	-0.060404	4.818625
301.653890	7999.809283	9.516186	-0.060465	4.818600
301.379257	7999.877043	9.521191	-0.060414	4.818621
301.728540	7999.756761	9.526195	-0.060479	4.818584
301.674306	7999.818976	9.531200	-0.060469	4.818602
301.356223	7999.883029	9.536205	-0.060410	4.818623
301.133099	7999.822472	9.541210	-0.060368	4.818605
301.139335	7999.876030	9.546215	-0.060369	4.818621
301.656536	7999.834465	9.551219	-0.060466	4.818607
301.376696	7999.780516	9.556224	-0.060413	4.818592
301.343643	7999.771698	9.561229	-0.060407	4.818590
301.773523	7999.865329	9.566234	-0.060487	4.818616
301.476482	7999.860443	9.571239	-0.060432	4.818615
301.903132	7999.776814	9.576243	-0.060511	4.818589
302.069514	7999.876483	9.581248	-0.060542	4.818618
302.290596	7999.969519	9.586253	-0.060584	4.818645
302.526668	7999.828899	9.591258	-0.060627	4.818602
302.178686	7999.834889	9.596263	-0.060563	4.818605
302.558781	7999.826162	9.601267	-0.060633	4.818601
302.537452	8000.015692	9.606272	-0.060629	4.818658
302.590403	7999.985962	9.611277	-0.060639	4.818649
302.500030	7999.849514	9.616282	-0.060622	4.818608
302.197443	7999.842458	9.621287	-0.060566	4.818607
302.300440	7999.847980	9.626291	-0.060585	4.818609
302.647335	7999.945788	9.631296	-0.060650	4.818636
302.486413	7999.913295	9.636301	-0.060620	4.818627
302.340271	7999.789761	9.641306	-0.060592	4.818591
302.487457	7999.879746	9.646311	-0.060620	4.818617
302.165046	7999.810564	9.651315	-0.060560	4.818598
301.946343	7999.811932	9.656320	-0.060519	4.818599
302.192755	7999.875932	9.661325	-0.060565	4.818617
302.486833	7999.869241	9.666330	-0.060619	4.818614
302.568332	7999.849317	9.671335	-0.060634	4.818608
302.352062	7999.851765	9.676339	-0.060594	4.818610
303.384802	7999.897611	9.681344	-0.060786	4.818619
302.648439	7999.848246	9.686349	-0.060649	4.818607
302.628178	7999.882587	9.691354	-0.060645	4.818618
302.878084	7999.816601	9.696359	-0.060692	4.818597
303.014799	7999.956788	9.701363	-0.060717	4.818638
302.915494	7999.849587	9.706368	-0.060699	4.818607
303.222771	7999.814753	9.711373	-0.060756	4.818595
303.027723	7999.861518	9.716378	-0.060720	4.818610
303.445510	8000.056725	9.721383	-0.060798	4.818666
302.781441	7999.846796	9.726387	-0.060674	4.818606
303.039261	7999.817614	9.731392	-0.060722	4.818597
303.156491	8000.083393	9.736397	-0.060744	4.818675
302.837796	7999.805569	9.741402	-0.060684	4.818594
302.792657	7999.986402	9.746407	-0.060676	4.818648
303.057209	7999.837760	9.751411	-0.060725	4.818603
303.214615	7999.912149	9.756416	-0.060754	4.818624
302.674282	7999.859025	9.761421	-0.060653	4.818610
302.966644	7999.863847	9.766426	-0.060708	4.818611
302.655491	7999.871361	9.771431	-0.060650	4.818614
302.788668	7999.824839	9.776435	-0.060675	4.818600
303.131071	7999.903715	9.781440	-0.060738	4.818622
303.105371	7999.867725	9.786445	-0.060734	4.818611
303.408540	7999.808719	9.791450	-0.060790	4.818593
303.300407	7999.970913	9.796455	-0.060770	4.818641
303.184023	7999.825738	9.801459	-0.060748	4.818599
303.494061	7999.959777	9.806464	-0.060806	4.818637
303.012300	7999.946208	9.811469	-0.060716	4.818635
302.973112	7999.796788	9.816474	-0.060709	4.818591
303.173795	7999.864395	9.821479	-0.060746	4.818610
303.121052	7999.837494	9.826483	-0.060736	4.818602
303.124844	7999.878439	9.831488	-0.060737	4.818615
303.427787	7999.801602	9.836493	-0.060793	4.818590
303.611854	7999.923527	9.841498	-0.060827	4.818626
303.623003	8000.130262	9.846503	-0.060830	4.818688
303.345370	7999.902250	9.851507	-0.060778	4.818621
303.717905	7999.950058	9.856512	-0.060847	4.818634
303.646874	7999.931310	9.861517	-0.060834	4.818628
303.817384	7999.981750	9.866522	-0.060866	4.818643
303.410457	7999.905178	9.871527	-0.060790	4.818621
303.708386	7999.846104	9.876531	-0.060845	4.818603
303.703495	7999.882742	9.881536	-0.060844	4.818614
303.252904	7999.863284	9.886541	-0.060760	4.818610
303.628021	7999.839814	9.891546	-0.060830	4.818601
303.123672	7999.909848	9.896551	-0.060736	4.818624
303.378581	7999.829244	9.901555	-0.060783	4.818599
303.520841	7999.889806	9.906560	-0.060810	4.818616
303.090372	7999.795104	9.911565	-0.060730	4.818590
303.516362	7999.869817	9.916570	-0.060809	4.818610
303.728285	7999.847385	9.921575	-0.060848	4.818603
303.715054	7999.796874	9.926579	-0.060846	4.818588
303.494925	8000.025786	9.931584	-0.060805	4.818657
303.524474	7999.938076	9.936589	-0.060810	4.818631
303.482497	7999.836857	9.941594	-0.060803	4.818601
303.218259	7999.771569	9.946599	-0.060753	4.818582
303.790099	7999.897455	9.951603	-0.060860	4.818618
303.814190	7999.887277	9.956608	-0.060864	4.818615
303.482927	7999.757152	9.961613	-0.060802	4.818577
303.717846	7999.923779	9.966618	-0.060846	4.818626
304.234065	7999.923108	9.971623	-0.060942	4.818624
303.918739	7999.925321	9.976627	-0.060884	4.818625
303.999940	7999.863446	9.981632	-0.060899	4.818607
304.378013	7999.953276	9.986637	-0.060969	4.818632
304.661108	7999.896108	9.991642	-0.061022	4.818614
304.443624	8000.170154	9.996647	-0.060981	4.818696
304.286646	8000.081078	10.001651	-0.060952	4.818670
304.474332	8000.030017	10.006656	-0.060987	4.818654
304.295227	8000.087475	10.011661	-0.060953	4.818672
304.610831	8000.008705	10.016666	-0.061012	4.818648
304.281502	8000.082049	10.021671	-0.060951	4.818671
304.028174	7999.818692	10.026675	-0.060903	4.818593
303.526772	7999.907641	10.031680	-0.060810	4.818622
303.901873	7999.821249	10.036685	-0.060880	4.818595
304.630177	7999.825417	10.041690	-0.061015	4.818593
304.132784	7999.974192	10.046695	-0.060923	4.818639
304.541333	7999.919695	10.051699	-0.060999	4.818621
304.386789	8000.011029	10.056704	-0.060970	4.818649
304.038375	7999.900603	10.061709	-0.060905	4.818618
304.078319	7999.837146	10.066714	-0.060912	4.818599
304.046021	7999.859797	10.071719	-0.060906	4.818605
304.363549	7999.890116	10.076723	-0.060966	4.818613
304.389358	7999.942883	10.081728	-0.060970	4.818629
304.433669	7999.874238	10.086733	-0.060979	4.818608
304.515590	7999.958142	10.091738	-0.060994	4.818633
303.632697	7999.917363	10.096743	-0.060829	4.818624
303.614520	7999.737801	10.101747	-0.060826	4.818571
304.239050	7999.854932	10.106752	-0.060942	4.818603
303.940914	7999.968530	10.111757	-0.060887	4.818638
303.478505	7999.800004	10.116762	-0.060800	4.818590
303.728307	7999.853566	10.121767	-0.060847	4.818605
303.911889	7999.829718	10.126771	-0.060881	4.818597
304.169036	7999.865549	10.131776	-0.060929	4.818607
303.855831	7999.853108	10.136781	-0.060870	4.818604
303.826034	7999.947103	10.141786	-0.060865	4.818632
303.765927	7999.771192	10.146791	-0.060854	4.818580
303.689817	7999.863539	10.151795	-0.060839	4.818608
303.943127	7999.828008	10.156800	-0.060887	4.818596
303.477996	7999.898549	10.161805	-0.060800	4.818619
303.454885	7999.856300	10.166810	-0.060796	4.818607
304.151799	7999.771970	10.171815	-0.060925	4.818579
303.892617	7999.886071	10.176819	-0.060877	4.818614
303.819938	7999.799136	10.181824	-0.060863	4.818588
303.853821	7999.925414	10.186829	-0.060870	4.818626
304.204050	7999.804095	10.191834	-0.060935	4.818588
303.760060	7999.815133	10.196839	-0.060852	4.818593
303.868489	7999.900427	10.201843	-0.060872	4.818618
303.840123	7999.847623	10.206848	-0.060867	4.818603
303.635049	7999.787293	10.211853	-0.060829	4.818586
303.647979	7999.822064	10.216858	-0.060831	4.818596
304.041765	7999.883779	10.221863	-0.060904	4.818613
304.039425	7999.797753	10.226867	-0.060904	4.818587
304.086341	7999.845548	10.231872	-0.060913	4.818601
304.053367	7999.881823	10.236877	-0.060906	4.818612
304.010970	7999.825692	10.241882	-0.060899	4.818595
303.972021	7999.899643	10.246887	-0.060891	4.818618
303.972169	7999.806308	10.251891	-0.060891	4.818590
304.347226	7999.784935	10.256896	-0.060961	4.818582
303.969708	7999.905897	10.261901	-0.060891	4.818620
304.001734	7999.799341	10.266906	-0.060897	4.818588
304.195056	7999.926632	10.271911	-0.060933	4.818625
304.190861	7999.846874	10.276915	-0.060932	4.818601
304.450211	7999.807227	10.281920	-0.060980	4.818588
304.656538	8000.043754	10.286925	-0.061019	4.818658
304.614977	7999.958268	10.291930	-0.061011	4.818633
303.957623	7999.806095	10.296935	-0.060888	4.818590
303.836544	7999.849621	10.301939	-0.060866	4.818603
304.270424	7999.825863	10.306944	-0.060946	4.818595
304.249072	7999.849704	10.311949	-0.060942	4.818602
304.188599	7999.785998	10.316954	-0.060931	4.818583
304.617051	7999.853407	10.321959	-0.061011	4.818601
304.455339	7999.769515	10.326963	-0.060981	4.818577
304.591602	7999.911800	10.331968	-0.061006	4.818619
304.466435	7999.880815	10.336973	-0.060983	4.818610
304.391945	7999.809586	10.341978	-0.060969	4.818589
304.532922	7999.877474	10.346983	-0.060995	4.818609
304.315110	7999.833756	10.351987	-0.060954	4.818597
304.756032	7999.856233	10.356992	-0.061036	4.818602
304.410876	7999.810869	10.361997	-0.060972	4.818590
304.250748	7999.843403	10.367002	-0.060942	4.818600
304.194443	7999.831137	10.372007	-0.060932	4.818596
304.276306	7999.819608	10.377011	-0.060947	4.818593
304.571304	7999.849636	10.382016	-0.061002	4.818600
304.356218	7999.880411	10.387021	-0.060962	4.818610
304.372174	7999.836569	10.392026	-0.060965	4.818597
304.249335	7999.806664	10.397031	-0.060942	4.818589
304.385278	7999.823100	10.402035	-0.060967	4.818593
304.528376	7999.943451	10.407040	-0.060994	4.818629
304.147326	7999.846236	10.412045	-0.060923	4.818601
303.971983	7999.914230	10.417050	-0.060890	4.818622
304.202795	7999.839607	10.422055	-0.060933	4.818599
304.626770	7999.838792	10.427059	-0.061012	4.818597
304.308164	7999.865083	10.432064	-0.060952	4.818606
304.184911	7999.863487	10.437069	-0.060929	4.818606
304.742730	7999.788896	10.442074	-0.061033	4.818582
304.682084	7999.826912	10.447079	-0.061022	4.818593
304.337083	7999.924173	10.452083	-0.060958	4.818624
304.379396	7999.797825	10.457088	-0.060965	4.818586
304.388455	7999.770673	10.462093	-0.060967	4.818578
304.266549	7999.811042	10.467098	-0.060944	4.818590
304.114919	7999.930729	10.472103	-0.060916	4.818626
304.650972	7999.749938	10.477107	-0.061016	4.818571
304.764354	7999.857320	10.482112	-0.061037	4.818602
304.562421	7999.805417	10.487117	-0.060999	4.818587
305.017305	7999.798711	10.492122	-0.061084	4.818584
305.181159	7999.924576	10.497127	-0.061114	4.818620
305.003895	7999.912842	10.502131	-0.061081	4.818618
304.789895	7999.850295	10.507136	-0.061041	4.818600
304.830177	7999.809914	10.512141	-0.061049	4.818588
304.939753	7999.852227	10.517146	-0.061069	4.818600
304.799488	7999.860898	10.522151	-0.061043	4.818603
305.163617	7999.900212	10.527155	-0.061111	4.818613
305.073696	7999.814100	10.532160	-0.061094	4.818588
304.140155	7999.864951	10.537165	-0.060920	4.818607
304.758733	7999.796389	10.542170	-0.061035	4.818584
304.506422	7999.848706	10.547175	-0.060988	4.818600
304.526339	7999.825889	10.552179	-0.060992	4.818594
304.854377	7999.884660	10.557184	-0.061053	4.818610
304.638600	7999.880819	10.562189	-0.061013	4.818610
304.576142	7999.852742	10.567194	-0.061001	4.818601
304.790400	7999.769515	10.572199	-0.061041	4.818576
305.069921	7999.827659	10.577203	-0.061093	4.818592
304.721676	7999.818959	10.582208	-0.061028	4.818591
304.766902	7999.892951	10.587213	-0.061037	4.818613
304.954980	7999.782119	10.592218	-0.061071	4.818579
304.702531	7999.843872	10.597223	-0.061024	4.818598
304.476737	7999.805295	10.602227	-0.060982	4.818588
304.418803	7999.876903	10.607232	-0.060972	4.818609
304.603837	7999.917046	10.612237	-0.061006	4.818620
304.742922	7999.806630	10.617242	-0.061032	4.818587
304.637353	7999.857698	10.622247	-0.061012	4.818603
305.089675	7999.819497	10.627251	-0.061096	4.818590
304.593508	7999.849784	10.632256	-0.061004	4.818600
304.583827	7999.885312	10.637261	-0.061002	4.818611
304.773658	7999.812257	10.642266	-0.061037	4.818589
304.331400	7999.814927	10.647271	-0.060955	4.818591
304.262672	7999.826620	10.652275	-0.060942	4.818595
304.626439	7999.879560	10.657280	-0.061010	4.818609
304.470970	7999.800992	10.662285	-0.060981	4.818586
304.873730	7999.798855	10.667290	-0.061056	4.818584
304.768421	7999.940115	10.672295	-0.061036	4.818627
304.597282	7999.809957	10.677299	-0.061004	4.818589
304.845795	7999.842531	10.682304	-0.061050	4.818597
304.775871	7999.926570	10.687309	-0.061037	4.818623
305.039717	7999.792597	10.692314	-0.061086	4.818582
304.675787	7999.834033	10.697319	-0.061019	4.818595
304.638441	7999.816768	10.702323	-0.061012	4.818590
304.324690	7999.863047	10.707328	-0.060953	4.818605
304.318427	7999.879742	10.712333	-0.060952	4.818610
304.555400	7999.871267	10.717338	-0.060996	4.818607
304.562086	7999.931127	10.722343	-0.060997	4.818625
304.411995	7999.857872	10.727347	-0.060969	4.818604
304.349024	7999.886419	10.732352	-0.060958	4.818612
304.635004	7999.835581	10.737357	-0.061011	4.818596
304.586824	7999.867465	10.742362	-0.061002	4.818606
304.458838	7999.871051	10.747367	-0.060978	4.818607
304.444543	7999.877156	10.752371	-0.060975	4.818609
304.453424	7999.916070	10.757376	-0.060977	4.818621
304.695957	7999.838452	10.762381	-0.061022	4.818597
304.801135	7999.887001	10.767386	-0.061041	4.818611
304.657914	7999.842150	10.772391	-0.061015	4.818598
304.721950	7999.871290	10.777395	-0.061027	4.818606
304.817316	7999.909225	10.782400	-0.061044	4.818617
304.705081	7999.910917	10.787405	-0.061023	4.818618
304.730881	7999.891323	10.792410	-0.061028	4.818612
304.709963	7999.851198	10.797415	-0.061024	4.818600
304.794710	7999.876412	10.802419	-0.061040	4.818608
304.643873	7999.889141	10.807424	-0.061012	4.818612
304.691343	7999.883459	10.812429	-0.061021	4.818610
304.839421	7999.868592	10.817434	-0.061048	4.818605
305.138064	7999.785407	10.822439	-0.061104	4.818579
305.192120	7999.881537	10.827443	-0.061114	4.818608
305.287380	7999.799917	10.832448	-0.061131	4.818583
305.448235	7999.914208	10.837453	-0.061161	4.818616
305.022476	7999.888773	10.842458	-0.061082	4.818610
305.248923	7999.803606	10.847463	-0.061124	4.818584
305.398994	7999.885247	10.852467	-0.061152	4.818608
305.197065	7999.846976	10.857472	-0.061114	4.818597
304.866182	7999.847938	10.862477	-0.061053	4.818599
304.842010	7999.839233	10.867482	-0.061048	4.818596
304.690144	7999.854047	10.872487	-0.061020	4.818601
304.621792	7999.840576	10.877491	-0.061007	4.818598
305.242270	7999.805598	10.882496	-0.061123	4.818585
305.326474	7999.926239	10.887501	-0.061138	4.818620
305.133516	7999.787407	10.892506	-0.061102	4.818580
305.395912	7999.850574	10.897511	-0.061151	4.818598
304.756949	7999.825530	10.902515	-0.061032	4.818593
305.053254	7999.871307	10.907520	-0.061087	4.818605
304.758162	7999.855953	10.912525	-0.061032	4.818602
305.165960	7999.918903	10.917530	-0.061108	4.818619
305.058367	7999.822075	10.922535	-0.061088	4.818590
304.844488	7999.829794	10.927539	-0.061048	4.818594
304.713672	7999.833343	10.932544	-0.061024	4.818595
305.176785	7999.870790	10.937549	-0.061110	4.818605
304.727333	7999.862878	10.942554	-0.061026	4.818604
304.873189	7999.823862	10.947559	-0.061053	4.818592
305.269169	7999.782835	10.952563	-0.061127	4.818578
305.602696	7999.875239	10.957568	-0.061189	4.818604
305.271073	7999.840534	10.962573	-0.061127	4.818595
305.319350	7999.821230	10.967578	-0.061136	4.818589
305.535618	7999.904776	10.972583	-0.061177	4.818613
305.187532	7999.865663	10.977587	-0.061112	4.818603
305.164888	7999.764691	10.982592	-0.061107	4.818573
305.190746	7999.878284	10.987597	-0.061112	4.818607
305.476487	7999.828492	10.992602	-0.061165	4.818591
305.274452	7999.813292	10.997607	-0.061128	4.818587
304.910766	7999.874655	11.002611	-0.061060	4.818607
305.044837	7999.879532	11.007616	-0.061085	4.818608
304.969601	7999.894287	11.012621	-0.061071	4.818612
305.599761	7999.810147	11.017626	-0.061188	4.818585
305.393381	7999.860960	11.022631	-0.061150	4.818601
305.623562	7999.802059	11.027635	-0.061193	4.818582
305.656799	7999.850728	11.032640	-0.061199	4.818597
305.537687	7999.916303	11.037645	-0.061177	4.818617
305.846799	7999.760891	11.042650	-0.061234	4.818569
305.213481	7999.971881	11.047655	-0.061116	4.818635
305.351177	7999.786986	11.052659	-0.061142	4.818579
305.318131	7999.828505	11.057664	-0.061135	4.818591
305.256046	7999.895867	11.062669	-0.061124	4.818612
305.312827	7999.834723	11.067674	-0.061134	4.818593
305.268133	7999.843581	11.072679	-0.061126	4.818596
305.627242	7999.752789	11.077683	-0.061193	4.818568
305.743915	7999.870704	11.082688	-0.061215	4.818602
305.905496	7999.815111	11.087693	-0.061245	4.818585
305.954073	7999.845101	11.092698	-0.061254	4.818594
306.121993	7999.887123	11.097703	-0.061285	4.818606
305.940504	7999.832335	11.102707	-0.061251	4.818590
305.503079	7999.853941	11.107712	-0.061169	4.818598
305.180936	7999.820408	11.112717	-0.061109	4.818590
305.273133	7999.895008	11.117722	-0.061127	4.818611
305.443175	7999.824843	11.122727	-0.061158	4.818590
304.911569	7999.875645	11.127731	-0.061059	4.818607
304.882300	7999.916164	11.132736	-0.061054	4.818619
305.189020	7999.845668	11.137741	-0.061111	4.818597
305.169427	7999.861143	11.142746	-0.061107	4.818602
305.279033	7999.917091	11.147751	-0.061127	4.818618
305.483800	7999.821157	11.152755	-0.061165	4.818589
306.187452	7999.817671	11.157760	-0.061296	4.818585
305.805802	7999.757148	11.162765	-0.061225	4.818568
305.827427	7999.867542	11.167770	-0.061229	4.818601
306.093525	7999.831130	11.172775	-0.061279	4.818589
306.017057	7999.950743	11.177779	-0.061265	4.818625
305.682546	7999.768128	11.182784	-0.061202	4.818572
305.783051	7999.827105	11.187789	-0.061221	4.818589
305.704569	7999.758968	11.192794	-0.061206	4.818569
305.724856	7999.899758	11.197799	-0.061210	4.818611
305.627076	7999.798861	11.202803	-0.061192	4.818581
306.108375	7999.924641	11.207808	-0.061281	4.818617
306.237993	7999.989241	11.212813	-0.061306	4.818636
305.916922	7999.926353	11.217818	-0.061246	4.818618
306.103843	7999.861649	11.222823	-0.061280	4.818598
306.187483	7999.896289	11.227827	-0.061296	4.818608
306.055987	7999.862073	11.232832	-0.061271	4.818599
306.097121	7999.802824	11.237837	-0.061279	4.818581
305.713779	7999.896444	11.242842	-0.061208	4.818610
305.816645	7999.789752	11.247847	-0.061227	4.818578
305.587210	7999.810902	11.252851	-0.061184	4.818585
305.866491	7999.817658	11.257856	-0.061236	4.818586
305.528931	7999.922357	11.262861	-0.061173	4.818619
305.766746	7999.807973	11.267866	-0.061217	4.818584
305.613310	7999.799693	11.272871	-0.061189	4.818582
305.819183	7999.844302	11.277875	-0.061227	4.818594
305.411316	7999.886217	11.282880	-0.061151	4.818608
305.391082	7999.882806	11.287885	-0.061147	4.818607
305.536504	7999.840638	11.292890	-0.061174	4.818594
305.989174	7999.845442	11.297895	-0.061258	4.818594
305.719989	7999.748620	11.302899	-0.061208	4.818566
306.054650	7999.838942	11.307904	-0.061271	4.818592
306.161232	7999.838221	11.312909	-0.061290	4.818591
305.876235	7999.783143	11.317914	-0.061237	4.818576
305.813494	7999.895592	11.322919	-0.061226	4.818610
305.571103	7999.815896	11.327923	-0.061180	4.818587
305.849585	7999.781741	11.332928	-0.061232	4.818576
305.755087	7999.903218	11.337933	-0.061215	4.818612
305.938464	7999.788129	11.342938	-0.061249	4.818577
305.691409	7999.918120	11.347943	-0.061203	4.818617
306.135630	7999.851501	11.352947	-0.061285	4.818595
306.227683	7999.772985	11.357952	-0.061302	4.818571
305.869214	7999.826025	11.362957	-0.061236	4.818589
306.157674	7999.807731	11.367962	-0.061289	4.818582
305.980722	7999.923946	11.372967	-0.061256	4.818617
306.183935	7999.717873	11.377971	-0.061294	4.818555
306.256851	7999.837321	11.382976	-0.061308	4.818590
305.917416	7999.886413	11.387981	-0.061244	4.818606
306.093958	7999.807941	11.392986	-0.061277	4.818582
306.270593	7999.889928	11.397991	-0.061310	4.818606
306.137259	7999.842055	11.402995	-0.061285	4.818592
306.082841	7999.889591	11.408000	-0.061275	4.818607
305.895197	7999.789628	11.413005	-0.061240	4.818578
306.139818	7999.878786	11.418010	-0.061286	4.818603
306.186983	7999.743057	11.423015	-0.061294	4.818563
306.038007	7999.927803	11.428019	-0.061267	4.818618
306.292431	7999.828315	11.433024	-0.061314	4.818588
305.834685	7999.757369	11.438029	-0.061229	4.818568
306.080978	7999.885352	11.443034	-0.061274	4.818605
305.906501	7999.796047	11.448039	-0.061242	4.818580
305.641801	7999.825131	11.453043	-0.061193	4.818589
306.292894	7999.823064	11.458048	-0.061314	4.818586
305.857407	7999.844694	11.463053	-0.061233	4.818594
306.021670	7999.868840	11.468058	-0.061263	4.818601
305.617252	7999.883531	11.473063	-0.061188	4.818607
305.490603	7999.901816	11.478067	-0.061164	4.818613
305.810016	7999.872386	11.483072	-0.061224	4.818603
305.743405	7999.870473	11.488077	-0.061211	4.818602
305.833633	7999.864296	11.493082	-0.061228	4.818600
306.002029	7999.912616	11.498087	-0.061259	4.818614
305.349870	7999.892641	11.503091	-0.061138	4.818610
305.118971	7999.905383	11.508096	-0.061095	4.818615
305.411332	7999.857774	11.513101	-0.061149	4.818600
305.707004	7999.830133	11.518106	-0.061204	4.818590
305.622921	7999.954891	11.523111	-0.061189	4.818628
305.623672	7999.809124	11.528115	-0.061189	4.818585
305.636630	7999.820825	11.533120	-0.061191	4.818588
305.631536	7999.893119	11.538125	-0.061190	4.818610
305.819502	7999.791723	11.543130	-0.061225	4.818579
305.582546	7999.843189	11.548135	-0.061181	4.818595
305.714222	7999.791404	11.553139	-0.061205	4.818579
306.094905	7999.906444	11.558144	-0.061276	4.818612
305.944348	7999.794375	11.563149	-0.061248	4.818579
305.982358	7999.804303	11.568154	-0.061255	4.818582
305.899316	7999.826298	11.573159	-0.061240	4.818589
306.119679	7999.870047	11.578163	-0.061281	4.818601
306.341076	7999.865568	11.583168	-0.061322	4.818599
305.983075	7999.874566	11.588173	-0.061255	4.818603
306.115058	7999.772446	11.593178	-0.061279	4.818572
306.147544	7999.878786	11.598183	-0.061286	4.818603
305.774019	7999.884438	11.603187	-0.061216	4.818606
305.744158	7999.869367	11.608192	-0.061210	4.818602
305.857146	7999.782732	11.613197	-0.061231	4.818576
305.928885	7999.871751	11.618202	-0.061245	4.818602
306.428747	7999.843607	11.623207	-0.061338	4.818592
306.042845	7999.770444	11.628211	-0.061266	4.818571
306.055460	7999.797871	11.633216	-0.061268	4.818580
305.836282	7999.852714	11.638221	-0.061227	4.818597
305.930333	7999.839245	11.643226	-0.061245	4.818592
306.253309	7999.809861	11.648231	-0.061305	4.818582
306.024337	7999.863528	11.653235	-0.061262	4.818599
306.358871	7999.743053	11.658240	-0.061324	4.818562
306.573175	7999.953476	11.663245	-0.061364	4.818624
306.212576	7999.784153	11.668250	-0.061297	4.818575
305.958798	7999.888888	11.673255	-0.061250	4.818607
306.110000	7999.752407	11.678259	-0.061278	4.818566
306.156639	7999.804396	11.683264	-0.061287	4.818581
306.213520	7999.932027	11.688269	-0.061297	4.818619
306.229689	7999.834700	11.693274	-0.061300	4.818590
306.208234	7999.813445	11.698279	-0.061296	4.818584
306.141368	7999.802090	11.703283	-0.061284	4.818581
306.161319	7999.844295	11.708288	-0.061287	4.818593
306.332317	7999.965014	11.713293	-0.061319	4.818628
306.223408	7999.825166	11.718298	-0.061299	4.818587
305.640341	7999.900471	11.723303	-0.061190	4.818612
306.012548	7999.809848	11.728307	-0.061259	4.818583
306.832082	7999.864497	11.733312	-0.061412	4.818596
306.326885	7999.840128	11.738317	-0.061318	4.818591
306.129749	7999.787235	11.743322	-0.061281	4.818576
306.284047	7999.888859	11.748327	-0.061310	4.818606
306.376096	7999.856488	11.753331	-0.061327	4.818596
306.315301	7999.802212	11.758336	-0.061315	4.818580
306.015794	7999.805676	11.763341	-0.061260	4.818582
306.261629	7999.854998	11.768346	-0.061305	4.818596
306.421192	7999.896913	11.773351	-0.061335	4.818608
306.399759	7999.816927	11.778355	-0.061331	4.818584
306.590108	7999.910630	11.783360	-0.061367	4.818611
306.393307	7999.784327	11.788365	-0.061330	4.818574
306.667463	7999.908479	11.793370	-0.061381	4.818610
306.322513	7999.826404	11.798375	-0.061317	4.818587
306.299097	7999.751638	11.803379	-0.061312	4.818565
306.065512	7999.947874	11.808384	-0.061269	4.818624
305.884141	7999.761996	11.813389	-0.061235	4.818570
306.403765	7999.858907	11.818394	-0.061331	4.818596
306.299522	7999.815606	11.823399	-0.061312	4.818584
306.246774	7999.887284	11.828403	-0.061302	4.818605
306.568555	7999.727840	11.833408	-0.061362	4.818557
306.401624	7999.825308	11.838413	-0.061331	4.818586
306.010730	7999.816053	11.843418	-0.061258	4.818585
306.323680	7999.844220	11.848423	-0.061316	4.818592
306.264246	7999.827717	11.853427	-0.061305	4.818588
306.129700	7999.894142	11.858432	-0.061280	4.818608
306.053152	7999.827078	11.863437	-0.061266	4.818588
306.242133	7999.727793	11.868442	-0.061301	4.818558
306.407236	7999.893530	11.873447	-0.061332	4.818607
306.260470	7999.790949	11.878451	-0.061304	4.818577
306.115301	7999.935892	11.883456	-0.061277	4.818620
306.166720	7999.775048	11.888461	-0.061287	4.818572
306.501823	7999.828672	11.893466	-0.061349	4.818587
306.345646	7999.787845	11.898471	-0.061320	4.818576
306.288850	7999.863665	11.903475	-0.061309	4.818598
306.394362	7999.809444	11.908480	-0.061329	4.818582
306.371383	7999.901434	11.913485	-0.061325	4.818609
306.265897	7999.808825	11.918490	-0.061305	4.818582
306.002130	7999.908187	11.923495	-0.061256	4.818613
305.565843	7999.836470	11.928499	-0.061175	4.818593
305.765893	7999.890442	11.933504	-0.061212	4.818608
305.778633	7999.815096	11.938509	-0.061214	4.818586
305.883629	7999.766112	11.943514	-0.061234	4.818571
306.119568	7999.865645	11.948519	-0.061278	4.818600
306.619514	7999.956012	11.953523	-0.061371	4.818625
306.526962	7999.805888	11.958528	-0.061353	4.818580
306.491280	7999.829545	11.963533	-0.061347	4.818587
306.467391	7999.740090	11.968538	-0.061342	4.818561
306.491346	7999.873588	11.973543	-0.061347	4.818600
306.345879	7999.826607	11.978547	-0.061319	4.818587
306.278892	7999.804762	11.983552	-0.061307	4.818581
306.451678	7999.901383	11.988557	-0.061339	4.818609
306.464901	7999.844918	11.993562	-0.061341	4.818592
306.580508	7999.810754	11.998567	-0.061363	4.818581
306.475744	7999.818834	12.003571	-0.061343	4.818584
306.245219	7999.829483	12.008576	-0.061300	4.818588
305.803328	7999.899272	12.013581	-0.061218	4.818611
306.002066	7999.811649	12.018586	-0.061255	4.818584
305.815210	7999.853276	12.023591	-0.061220	4.818597
305.732411	7999.768304	12.028595	-0.061205	4.818572
305.992179	7999.826195	12.033600	-0.061253	4.818588
306.077442	7999.891269	12.038605	-0.061269	4.818607
306.215783	7999.843765	12.043610	-0.061295	4.818593
306.215368	7999.829074	12.048615	-0.061295	4.818588
305.928599	7999.861019	12.053619	-0.061241	4.818599
306.114508	7999.943126	12.058624	-0.061276	4.818623
305.866868	7999.783657	12.063629	-0.061230	4.818576
306.312088	7999.813535	12.068634	-0.061312	4.818583
305.995524	7999.877604	12.073639	-0.061253	4.818604
305.849464	7999.865225	12.078643	-0.061226	4.818600
305.879963	7999.865616	12.083648	-0.061232	4.818600
305.804589	7999.830030	12.088653	-0.061218	4.818590
305.854116	7999.812840	12.093658	-0.061227	4.818585
305.918546	7999.954202	12.098663	-0.061239	4.818627
305.806524	7999.895069	12.103667	-0.061218	4.818610
305.800391	7999.889743	12.108672	-0.061217	4.818608
305.926990	7999.806430	12.113677	-0.061240	4.818583
305.906529	7999.830284	12.118682	-0.061236	4.818590
305.532527	7999.912488	12.123687	-0.061167	4.818616
305.770072	7999.837951	12.128691	-0.061211	4.818593
305.967570	7999.849942	12.133696	-0.061248	4.818595
306.011041	7999.923914	12.138701	-0.061256	4.818617
306.573356	7999.754997	12.143706	-0.061360	4.818565
306.017375	7999.906161	12.148711	-0.061257	4.818612
306.210296	7999.698907	12.153715	-0.061293	4.818550
306.148520	7999.909950	12.158720	-0.061281	4.818613
306.282940	7999.762765	12.163725	-0.061306	4.818568
306.155272	7999.870180	12.168730	-0.061282	4.818601
306.239841	7999.923709	12.173735	-0.061298	4.818616
306.086415	7999.792725	12.178739	-0.061269	4.818578
306.104472	7999.822321	12.183744	-0.061273	4.818587
306.377190	7999.885625	12.188749	-0.061324	4.818605
305.899361	7999.796590	12.193754	-0.061235	4.818580
306.161566	7999.809417	12.198759	-0.061283	4.818583
306.168127	7999.897594	12.203763	-0.061285	4.818609
306.433285	7999.755246	12.208768	-0.061334	4.818566
306.400881	7999.920527	12.213773	-0.061328	4.818615
306.306571	7999.733675	12.218778	-0.061310	4.818560
306.565164	7999.947818	12.223783	-0.061358	4.818622
306.446856	7999.850847	12.228787	-0.061336	4.818594
306.441301	7999.815115	12.233792	-0.061335	4.818583
306.365762	7999.774282	12.238797	-0.061321	4.818571
306.651777	7999.893343	12.243802	-0.061374	4.818606
306.680162	7999.973414	12.248807	-0.061380	4.818630
306.248238	7999.823093	12.253811	-0.061299	4.818586
306.205871	7999.885467	12.258816	-0.061291	4.818605
306.076033	7999.849176	12.263821	-0.061267	4.818595
306.110731	7999.847524	12.268826	-0.061273	4.818594
306.100191	7999.866263	12.273831	-0.061271	4.818600
306.136479	7999.874071	12.278835	-0.061278	4.818602
306.037843	7999.897961	12.283840	-0.061260	4.818610
306.011358	7999.891323	12.288845	-0.061255	4.818608
306.016059	7999.881943	12.293850	-0.061256	4.818605
306.242902	7999.833487	12.298855	-0.061298	4.818590
306.240638	7999.875404	12.303859	-0.061297	4.818602
306.657682	7999.759143	12.308864	-0.061375	4.818566
306.339498	7999.881922	12.313869	-0.061316	4.818604
306.337613	7999.770727	12.318874	-0.061315	4.818571
306.432630	7999.922974	12.323879	-0.061333	4.818615
306.014258	7999.845194	12.328883	-0.061255	4.818594
306.267416	7999.830638	12.333888	-0.061302	4.818589
306.398569	7999.853307	12.338893	-0.061326	4.818595
306.672461	7999.783436	12.343898	-0.061377	4.818573
306.805742	7999.782012	12.348903	-0.061402	4.818572
306.908410	7999.844166	12.353907	-0.061421	4.818590
306.935341	7999.838219	12.358912	-0.061426	4.818588
306.655302	7999.885981	12.363917	-0.061374	4.818604
306.622020	7999.740820	12.368922	-0.061368	4.818561
306.430981	7999.854756	12.373927	-0.061332	4.818595
306.219247	7999.818454	12.378931	-0.061293	4.818585
306.370487	7999.858163	12.383936	-0.061321	4.818596
306.366849	7999.888527	12.388941	-0.061320	4.818605
306.544306	7999.833139	12.393946	-0.061353	4.818588
306.472194	7999.838495	12.398951	-0.061340	4.818590
306.365785	7999.822433	12.403955	-0.061320	4.818586
306.196428	7999.909383	12.408960	-0.061288	4.818612
306.189280	7999.894605	12.413965	-0.061287	4.818608
305.953360	7999.919866	12.418970	-0.061243	4.818616
306.145864	7999.906623	12.423975	-0.061279	4.818612
306.341934	7999.885036	12.428979	-0.061315	4.818605
306.117051	7999.877928	12.433984	-0.061273	4.818603
305.993858	7999.866893	12.438989	-0.061250	4.818600
306.420899	7999.866123	12.443994	-0.061330	4.818599
306.368066	7999.894801	12.448999	-0.061320	4.818607
306.394416	7999.815435	12.454003	-0.061325	4.818584
306.835389	7999.808553	12.459008	-0.061407	4.818580
306.597297	7999.818054	12.464013	-0.061362	4.818584
306.777326	7999.828771	12.469018	-0.061396	4.818586
306.647743	7999.854359	12.474023	-0.061372	4.818594
306.520260	7999.833829	12.479027	-0.061348	4.818589
306.451455	7999.979762	12.484032	-0.061335	4.818632
306.237484	7999.849042	12.489037	-0.061295	4.818594
306.268391	7999.859927	12.494042	-0.061301	4.818597
306.120159	7999.929321	12.499047	-0.061273	4.818619
305.851632	7999.921649	12.504051	-0.061223	4.818617
306.106924	7999.925998	12.509056	-0.061271	4.818618
305.856005	7999.910163	12.514061	-0.061224	4.818614
305.829930	7999.921359	12.519066	-0.061219	4.818617
306.040199	7999.907297	12.524071	-0.061258	4.818612
306.176396	7999.866058	12.529075	-0.061283	4.818600
306.231338	7999.888790	12.534080	-0.061294	4.818606
306.286380	7999.890548	12.539085	-0.061304	4.818606
306.340026	7999.946823	12.544090	-0.061314	4.818623
306.254608	7999.928935	12.549095	-0.061298	4.818618
306.054579	7999.916905	12.554099	-0.061261	4.818615
306.122310	7999.960778	12.559104	-0.061273	4.818628
306.217054	7999.944172	12.564109	-0.061291	4.818623
306.087151	7999.941440	12.569114	-0.061267	4.818622
306.036720	7999.905127	12.574119	-0.061257	4.818612
306.075379	7999.924502	12.579123	-0.061264	4.818617
306.119875	7999.945001	12.584128	-0.061273	4.818623
305.845650	7999.903695	12.589133	-0.061221	4.818612
305.990262	7999.943318	12.594138	-0.061248	4.818623
306.208421	7999.942992	12.599143	-0.061289	4.818622
306.290410	7999.910490	12.604147	-0.061304	4.818612
306.224467	7999.927463	12.609152	-0.061292	4.818618
306.352653	7999.907095	12.614157	-0.061316	4.818611
306.432384	7999.920709	12.619162	-0.061330	4.818615
306.539881	7999.890635	12.624167	-0.061350	4.818605
306.676030	7999.841005	12.629171	-0.061376	4.818590
306.562600	7999.884631	12.634176	-0.061355	4.818604
306.582304	7999.855518	12.639181	-0.061358	4.818595
306.887144	7999.880436	12.644186	-0.061415	4.818601
307.013102	7999.845357	12.649191	-0.061438	4.818590
306.820815	7999.829231	12.654195	-0.061402	4.818586
307.062914	7999.860679	12.659200	-0.061448	4.818595
306.891841	7999.764073	12.664205	-0.061416	4.818566
306.953073	7999.876032	12.669210	-0.061427	4.818600
306.807516	7999.832195	12.674215	-0.061400	4.818587
306.840781	7999.895548	12.679219	-0.061406	4.818606
306.727331	7999.847931	12.684224	-0.061385	4.818592
306.597918	7999.839961	12.689229	-0.061361	4.818590
306.647008	7999.828009	12.694234	-0.061370	4.818586
306.803305	7999.830029	12.699239	-0.061399	4.818586
306.564722	7999.897205	12.704243	-0.061354	4.818607
307.427640	7999.817129	12.709248	-0.061515	4.818580
307.078306	7999.865043	12.714253	-0.061450	4.818596
307.028829	7999.878033	12.719258	-0.061441	4.818600
306.993216	7999.799961	12.724263	-0.061434	4.818577
307.041737	7999.845683	12.729267	-0.061443	4.818590
306.938215	7999.790854	12.734272	-0.061424	4.818574
306.964672	7999.898167	12.739277	-0.061429	4.818606
306.981737	7999.821825	12.744282	-0.061432	4.818583
307.225066	7999.793509	12.749287	-0.061477	4.818574
306.935934	7999.849544	12.754291	-0.061423	4.818592
307.195633	7999.927365	12.759296	-0.061471	4.818614
306.901564	7999.814484	12.764301	-0.061417	4.818581
306.675667	7999.812607	12.769306	-0.061375	4.818582
306.761664	7999.839936	12.774311	-0.061390	4.818590
306.929400	7999.874615	12.779315	-0.061422	4.818599
306.788934	7999.843429	12.784320	-0.061395	4.818590
306.646024	7999.911844	12.789325	-0.061369	4.818611
307.098426	7999.790796	12.794330	-0.061453	4.818574
307.250463	7999.932248	12.799335	-0.061481	4.818615
307.029536	7999.820313	12.804339	-0.061440	4.818583
306.921630	7999.857718	12.809344	-0.061420	4.818594
307.020706	7999.815998	12.814349	-0.061438	4.818581
307.075300	7999.893262	12.819354	-0.061449	4.818604
306.777969	7999.806559	12.824359	-0.061393	4.818580
306.973766	7999.833211	12.829363	-0.061430	4.818587
307.008031	7999.797994	12.834368	-0.061436	4.818576
306.805943	7999.797474	12.839373	-0.061398	4.818577
306.739192	7999.820728	12.844378	-0.061386	4.818584
307.158554	7999.888031	12.849383	-0.061464	4.818602
306.787787	7999.884277	12.854387	-0.061395	4.818603
306.721313	7999.843561	12.859392	-0.061382	4.818591
306.701143	7999.806591	12.864397	-0.061378	4.818580
306.816055	7999.843733	12.869402	-0.061400	4.818590
306.874931	7999.872809	12.874407	-0.061411	4.818599
306.531244	7999.864163	12.879411	-0.061347	4.818598
306.650935	7999.898221	12.884416	-0.061369	4.818607
306.233090	7999.924273	12.889421	-0.061291	4.818617
306.727802	7999.818456	12.894426	-0.061383	4.818583
306.780947	7999.942894	12.899431	-0.061393	4.818620
306.829837	7999.793552	12.904435	-0.061402	4.818576
306.709522	7999.850722	12.909440	-0.061380	4.818593
306.406605	7999.885603	12.914445	-0.061323	4.818605
306.538547	7999.840114	12.919450	-0.061348	4.818590
306.820185	7999.824878	12.924455	-0.061400	4.818585
306.742836	7999.814436	12.929459	-0.061386	4.818582
306.853594	7999.960596	12.934464	-0.061406	4.818625
306.584105	7999.838595	12.939469	-0.061356	4.818590
306.661061	7999.829100	12.944474	-0.061370	4.818587
306.925650	7999.834619	12.949479	-0.061420	4.818587
306.775277	7999.842109	12.954483	-0.061392	4.818590
307.181047	7999.758214	12.959488	-0.061467	4.818564
306.746401	7999.921436	12.964493	-0.061386	4.818614
306.953560	7999.733240	12.969498	-0.061425	4.818557
306.997183	7999.905799	12.974503	-0.061433	4.818608
306.715444	7999.765811	12.979507	-0.061380	4.818568
306.519012	7999.878629	12.984512	-0.061344	4.818602
306.772246	7999.879806	12.989517	-0.061391	4.818601
306.710032	7999.811878	12.994522	-0.061379	4.818581
306.584362	7999.819687	12.999527	-0.061356	4.818584
306.438062	7999.950983	13.004531	-0.061328	4.818624
306.550829	7999.882173	13.009536	-0.061349	4.818603
306.498187	7999.908757	13.014541	-0.061340	4.818611
306.526484	7999.939534	13.019546	-0.061345	4.818620
306.463579	7999.896767	13.024551	-0.061333	4.818608
306.484925	7999.869773	13.029555	-0.061337	4.818600
306.772553	7999.887126	13.034560	-0.061390	4.818604
306.891600	7999.858250	13.039565	-0.061413	4.818595
307.578522	7999.731848	13.044570	-0.061540	4.818554
307.206354	7999.971391	13.049575	-0.061471	4.818627
307.061553	7999.868832	13.054579	-0.061444	4.818597
307.010217	7999.896481	13.059584	-0.061435	4.818605
306.555137	7999.902125	13.064589	-0.061350	4.818609
306.717606	7999.900030	13.069594	-0.061380	4.818608
306.971313	7999.825702	13.074599	-0.061427	4.818585
306.766962	7999.828298	13.079603	-0.061389	4.818586
307.062019	7999.841553	13.084608	-0.061444	4.818589
306.771359	7999.884983	13.089613	-0.061390	4.818603
307.410415	7999.871228	13.094618	-0.061509	4.818596
307.409735	7999.924704	13.099623	-0.061509	4.818612
307.457072	7999.889656	13.104627	-0.061517	4.818602
307.133515	7999.856099	13.109632	-0.061457	4.818593
306.914528	7999.878432	13.114637	-0.061416	4.818600
306.984915	7999.904511	13.119642	-0.061429	4.818608
307.311441	7999.841613	13.124647	-0.061490	4.818588
306.527432	7999.924803	13.129651	-0.061344	4.818616
306.700436	7999.936478	13.134656	-0.061376	4.818619
306.648796	7999.893856	13.139661	-0.061367	4.818606
306.549537	7999.900959	13.144666	-0.061348	4.818609
306.902473	7999.852037	13.149671	-0.061414	4.818593
306.870506	7999.847426	13.154675	-0.061408	4.818591
306.918036	7999.832307	13.159680	-0.061417	4.818587
307.076493	7999.950768	13.164685	-0.061446	4.818621
307.080117	7999.844887	13.169690	-0.061447	4.818590
306.986338	7999.865694	13.174695	-0.061429	4.818596
307.123010	7999.763633	13.179699	-0.061454	4.818566
307.248066	7999.836565	13.184704	-0.061478	4.818587
307.089769	7999.832415	13.189709	-0.061448	4.818586
307.094035	7999.805200	13.194714	-0.061449	4.818578
306.942177	7999.997253	13.199719	-0.061421	4.818636
307.046840	7999.841290	13.204723	-0.061440	4.818589
306.988321	7999.900310	13.209728	-0.061429	4.818607
307.387477	7999.842548	13.214733	-0.061504	4.818588
307.047905	7999.870661	13.219738	-0.061440	4.818598
307.289263	7999.851759	13.224743	-0.061485	4.818591
306.985106	7999.814258	13.229747	-0.061428	4.818581
307.239453	7999.834328	13.234752	-0.061476	4.818586
307.047673	7999.957695	13.239757	-0.061440	4.818624
306.893038	7999.872838	13.244762	-0.061411	4.818599
306.785881	7999.860960	13.249767	-0.061391	4.818596
307.076467	7999.841646	13.254771	-0.061445	4.818589
307.303675	7999.876047	13.259776	-0.061488	4.818598
307.117734	7999.843223	13.264781	-0.061453	4.818589
306.856156	7999.878639	13.269786	-0.061404	4.818601
306.930544	7999.906867	13.274791	-0.061418	4.818609
306.807900	7999.881155	13.279795	-0.061395	4.818602
306.785519	7999.899740	13.284800	-0.061391	4.818607
307.166240	7999.854325	13.289805	-0.061462	4.818592
307.105107	7999.844092	13.294810	-0.061450	4.818590
307.513129	7999.790640	13.299815	-0.061526	4.818572
307.162275	7999.936069	13.304819	-0.061461	4.818617
307.289813	7999.861157	13.309824	-0.061485	4.818594
307.097428	7999.880688	13.314829	-0.061449	4.818600
307.190203	7999.857765	13.319834	-0.061466	4.818593
307.045071	7999.887346	13.324839	-0.061439	4.818603
307.176692	7999.813536	13.329843	-0.061463	4.818580
307.469013	7999.822561	13.334848	-0.061518	4.818582
307.200391	7999.901934	13.339853	-0.061468	4.818606
307.407344	7999.772465	13.344858	-0.061506	4.818567
307.064090	7999.857164	13.349863	-0.061442	4.818594
307.281559	7999.814880	13.354867	-0.061483	4.818580
307.900414	7999.801913	13.359872	-0.061598	4.818574
307.537891	7999.905241	13.364877	-0.061530	4.818606
307.199450	7999.879881	13.369882	-0.061467	4.818600
307.493982	7999.826009	13.374887	-0.061522	4.818583
307.138160	7999.841326	13.379891	-0.061456	4.818589
307.373378	7999.847515	13.384896	-0.061500	4.818590
307.328059	7999.862657	13.389901	-0.061491	4.818594
307.354261	7999.908091	13.394906	-0.061496	4.818608
307.347644	7999.824100	13.399911	-0.061495	4.818583
307.105779	7999.840893	13.404915	-0.061450	4.818589
307.163513	7999.859467	13.409920	-0.061460	4.818594
307.143965	7999.831943	13.414925	-0.061457	4.818586
306.860648	7999.933149	13.419930	-0.061404	4.818617
307.436306	7999.844112	13.424935	-0.061511	4.818588
307.110221	7999.844083	13.429939	-0.061450	4.818590
307.571360	7999.809148	13.434944	-0.061536	4.818577
307.647550	7999.921302	13.439949	-0.061550	4.818610
307.450926	7999.856876	13.444954	-0.061513	4.818592
307.618358	7999.873723	13.449959	-0.061545	4.818596
307.826911	7999.758958	13.454963	-0.061583	4.818561
307.763304	7999.842034	13.459968	-0.061572	4.818586
307.717240	7999.845630	13.464973	-0.061563	4.818588
307.700460	7999.850653	13.469978	-0.061560	4.818589
308.079821	7999.834588	13.474983	-0.061630	4.818583
307.259616	7999.832355	13.479987	-0.061478	4.818586
307.577033	7999.827023	13.484992	-0.061537	4.818583
307.483044	7999.847827	13.489997	-0.061519	4.818589
307.510096	7999.799931	13.495002	-0.061524	4.818575
307.580947	7999.880553	13.500007	-0.061537	4.818599
307.891499	7999.800669	13.505011	-0.061595	4.818574
308.453518	7999.955825	13.510016	-0.061700	4.818618
308.062514	7999.828048	13.515021	-0.061627	4.818581
307.863848	7999.770936	13.520026	-0.061590	4.818565
308.563636	7999.793630	13.525031	-0.061720	4.818569
308.165201	7999.962567	13.530035	-0.061646	4.818621
307.899607	7999.828025	13.535040	-0.061596	4.818582
308.060585	7999.757741	13.540045	-0.061626	4.818560
307.673629	7999.880679	13.545050	-0.061554	4.818598
307.987853	7999.807135	13.550055	-0.061613	4.818575
307.634000	7999.888551	13.555059	-0.061547	4.818601
307.771434	7999.823205	13.560064	-0.061572	4.818581
307.992631	7999.741115	13.565069	-0.061613	4.818556
307.846361	7999.878707	13.570074	-0.061586	4.818597
307.874280	7999.815090	13.575079	-0.061591	4.818578
307.642729	7999.812089	13.580083	-0.061548	4.818578
307.806323	7999.810009	13.585088	-0.061579	4.818577
307.717019	7999.922118	13.590093	-0.061562	4.818610
307.978842	7999.826920	13.595098	-0.061611	4.818581
308.081263	7999.817756	13.600103	-0.061630	4.818578
307.820183	7999.867860	13.605107	-0.061581	4.818594
308.271646	7999.805533	13.610112	-0.061665	4.818574
308.004114	7999.783188	13.615117	-0.061615	4.818568
307.947307	7999.817059	13.620122	-0.061604	4.818578
307.732372	7999.819517	13.625127	-0.061564	4.818580
307.919016	7999.863883	13.630131	-0.061599	4.818592
307.995735	7999.832361	13.635136	-0.061613	4.818583
308.114709	7999.884241	13.640141	-0.061636	4.818598
308.260520	7999.888224	13.645146	-0.061663	4.818598
307.943039	7999.952281	13.650151	-0.061604	4.818619
307.754989	7999.833427	13.655155	-0.061568	4.818584
307.738731	7999.854190	13.660160	-0.061565	4.818590
308.029175	7999.845363	13.665165	-0.061619	4.818586
308.115443	7999.787745	13.670170	-0.061635	4.818569
308.812715	7999.907947	13.675175	-0.061765	4.818602
308.747711	7999.799075	13.680179	-0.061753	4.818570
308.929320	7999.941965	13.685184	-0.061787	4.818612
308.495980	7999.994032	13.690189	-0.061706	4.818629
308.592867	7999.904039	13.695194	-0.061724	4.818602
308.205987	7999.825608	13.700199	-0.061652	4.818580
308.017091	7999.858818	13.705203	-0.061617	4.818590
308.158177	7999.835472	13.710208	-0.061643	4.818583
307.728949	7999.820472	13.715213	-0.061563	4.818580
307.942354	7999.860988	13.720218	-0.061603	4.818591
307.780568	7999.835817	13.725223	-0.061573	4.818585
307.274583	7999.886946	13.730227	-0.061478	4.818602
307.712831	7999.820252	13.735232	-0.061560	4.818580
307.849425	7999.770627	13.740237	-0.061585	4.818565
307.754025	7999.895243	13.745242	-0.061568	4.818602
307.643660	7999.879128	13.750247	-0.061547	4.818598
307.720037	7999.818236	13.755251	-0.061561	4.818580
307.471560	7999.890528	13.760256	-0.061515	4.818602
307.899880	7999.838389	13.765261	-0.061595	4.818585
307.570712	7999.910685	13.770266	-0.061533	4.818608
308.100831	7999.853571	13.775271	-0.061632	4.818589
308.073483	7999.921386	13.780275	-0.061627	4.818609
307.693185	7999.878701	13.785280	-0.061556	4.818598
307.627985	7999.818074	13.790285	-0.061544	4.818580
307.838179	7999.788280	13.795290	-0.061583	4.818570
307.536537	7999.922811	13.800295	-0.061527	4.818611
307.599609	7999.853357	13.805299	-0.061538	4.818590
307.719964	7999.854912	13.810304	-0.061561	4.818590
307.733992	7999.867676	13.815309	-0.061563	4.818594
307.503035	7999.844756	13.820314	-0.061520	4.818588
307.625887	7999.866271	13.825319	-0.061543	4.818594
307.313934	7999.877961	13.830323	-0.061485	4.818599
307.720157	7999.859096	13.835328	-0.061561	4.818592
307.526290	7999.875461	13.840333	-0.061524	4.818597
307.387807	7999.898836	13.845338	-0.061499	4.818605
307.879088	7999.860097	13.850343	-0.061590	4.818591
307.889843	7999.835062	13.855347	-0.061592	4.818584
307.781018	7999.880846	13.860352	-0.061572	4.818598
307.779338	7999.935358	13.865357	-0.061571	4.818614
307.288132	7999.925848	13.870362	-0.061480	4.818613
307.354808	7999.912026	13.875367	-0.061492	4.818609
307.351594	7999.903591	13.880371	-0.061492	4.818606
307.660030	7999.874021	13.885376	-0.061549	4.818596
307.787016	7999.807492	13.890381	-0.061572	4.818576
307.743264	7999.756582	13.895386	-0.061564	4.818561
308.116361	7999.913484	13.900391	-0.061634	4.818606
308.082269	7999.759916	13.905395	-0.061627	4.818561
307.745884	7999.865680	13.910400	-0.061565	4.818594
308.094083	7999.763210	13.915405	-0.061629	4.818562
308.529585	7999.927216	13.920410	-0.061711	4.818609
308.438642	7999.826399	13.925415	-0.061694	4.818579
307.687905	7999.827162	13.930419	-0.061554	4.818582
307.498700	7999.836246	13.935424	-0.061518	4.818586
307.879867	7999.850618	13.940429	-0.061589	4.818589
308.090844	7999.791469	13.945434	-0.061629	4.818570
308.529836	7999.811834	13.950439	-0.061710	4.818575
308.243314	7999.847975	13.955443	-0.061657	4.818586
308.110503	7999.845203	13.960448	-0.061632	4.818586
308.208105	7999.865343	13.965453	-0.061650	4.818592
308.085972	7999.813416	13.970458	-0.061628	4.818577
308.045681	7999.746818	13.975463	-0.061620	4.818557
308.040175	7999.936575	13.980467	-0.061619	4.818614
308.600879	7999.793857	13.985472	-0.061723	4.818569
308.196539	7999.846301	13.990477	-0.061648	4.818586
308.256123	7999.837631	13.995482	-0.061659	4.818583
308.234928	7999.906574	14.000487	-0.061655	4.818604
308.302812	7999.884377	14.005491	-0.061668	4.818597
308.631379	7999.739701	14.010496	-0.061729	4.818553
308.399461	7999.856257	14.015501	-0.061686	4.818588
308.425118	7999.810439	14.020506	-0.061690	4.818575
308.476511	7999.828932	14.025511	-0.061700	4.818580
307.770868	7999.895303	14.030515	-0.061568	4.818602
307.882646	7999.854796	14.035520	-0.061589	4.818590
307.966317	7999.857974	14.040525	-0.061605	4.818590
308.488621	7999.847956	14.045530	-0.061702	4.818586
307.776968	7999.879639	14.050535	-0.061569	4.818598
307.575664	7999.827737	14.055539	-0.061532	4.818583
307.742069	7999.830938	14.060544	-0.061563	4.818583
307.691260	7999.947740	14.065549	-0.061553	4.818618
307.708422	7999.813716	14.070554	-0.061556	4.818578
308.178048	7999.816648	14.075559	-0.061644	4.818577
307.802785	7999.787664	14.080563	-0.061574	4.818570
308.144794	7999.904310	14.085568	-0.061638	4.818604
308.089864	7999.806058	14.090573	-0.061627	4.818575
307.735325	7999.859148	14.095578	-0.061561	4.818592
308.318786	7999.816359	14.100583	-0.061670	4.818577
307.611183	7999.851242	14.105587	-0.061538	4.818590
307.595058	7999.856275	14.110592	-0.061535	4.818591
307.808334	7999.971253	14.115597	-0.061575	4.818625
307.874283	7999.783323	14.120602	-0.061587	4.818569
307.854498	7999.838650	14.125607	-0.061583	4.818585
307.710919	7999.866154	14.130611	-0.061556	4.818594
308.140848	7999.810889	14.135616	-0.061636	4.818576
307.604367	7999.989574	14.140621	-0.061537	4.818631
307.481478	7999.831712	14.145626	-0.061514	4.818585
307.881725	7999.866257	14.150631	-0.061588	4.818593
307.884527	7999.823290	14.155635	-0.061589	4.818581
307.855795	7999.837598	14.160640	-0.061583	4.818585
308.023558	7999.886964	14.165645	-0.061614	4.818599
307.772721	7999.810298	14.170650	-0.061568	4.818577
307.717512	7999.903970	14.175655	-0.061557	4.818605
307.727049	7999.852701	14.180659	-0.061559	4.818590
308.002024	7999.869893	14.185664	-0.061610	4.818594
307.814536	7999.867462	14.190669	-0.061575	4.818594
307.746551	7999.794213	14.195674	-0.061563	4.818572
307.663256	7999.888571	14.200679	-0.061547	4.818601
307.806160	7999.847419	14.205683	-0.061574	4.818588
307.861614	7999.865963	14.210688	-0.061584	4.818593
307.588812	7999.897038	14.215693	-0.061533	4.818604
307.712651	7999.898638	14.220698	-0.061556	4.818604
307.436706	7999.884575	14.225703	-0.061505	4.818600
307.832702	7999.816285	14.230707	-0.061578	4.818579
307.777855	7999.888987	14.235712	-0.061568	4.818600
307.805877	7999.855786	14.240717	-0.061573	4.818590
307.678609	7999.803794	14.245722	-0.061549	4.818576
307.889608	7999.888328	14.250727	-0.061589	4.818600
308.037650	7999.838852	14.255731	-0.061616	4.818585
307.691233	7999.914071	14.260736	-0.061552	4.818608
307.458194	7999.946709	14.265741	-0.061508	4.818619
307.771358	7999.928737	14.270746	-0.061567	4.818612
308.044397	7999.870392	14.275751	-0.061617	4.818594
307.707238	7999.935242	14.280755	-0.061555	4.818615
307.568311	7999.913514	14.285760	-0.061529	4.818609
307.505925	7999.902215	14.290765	-0.061517	4.818605
307.436844	7999.895026	14.295770	-0.061504	4.818604
307.478561	7999.923880	14.300775	-0.061512	4.818612
307.707893	7999.837700	14.305779	-0.061554	4.818586
307.709026	7999.582861	14.310784	-0.061554	4.818510

307.503847	7996.476181	14.315789	-0.061514	4.817586
307.996219	7990.796084	14.320794	-0.061602	4.815892
307.929982	7984.175141	14.325799	-0.061585	4.813920
308.177077	7976.798379	14.330803	-0.061627	4.811721
307.832886	7969.171692	14.335808	-0.061558	4.809448
307.886203	7961.424830	14.340813	-0.061562	4.807136
307.841242	7953.403389	14.345818	-0.061549	4.804743
307.867641	7945.630346	14.350823	-0.061549	4.802421
307.625569	7937.607248	14.355827	-0.061498	4.800025
307.619000	7929.620146	14.360832	-0.061492	4.797638
307.128570	7921.664035	14.365837	-0.061395	4.795260
307.053956	7913.596620	14.370842	-0.061376	4.792846
307.068921	7905.594734	14.375847	-0.061373	4.790451
306.770763	7897.615458	14.380851	-0.061313	4.788062
306.802881	7889.578063	14.385856	-0.061313	4.785653
306.928496	7881.564392	14.390861	-0.061332	4.783250
307.388725	7873.518478	14.395866	-0.061412	4.780835
307.352890	7865.569413	14.400871	-0.061400	4.778450
307.104244	7857.530842	14.405875	-0.061349	4.776037
307.141593	7849.570789	14.410880	-0.061350	4.773646
306.786728	7841.595567	14.415885	-0.061279	4.771249
306.928057	7833.471161	14.420890	-0.061300	4.768806
307.390535	7825.568414	14.425895	-0.061381	4.766427
307.159897	7817.512146	14.430899	-0.061333	4.764002
307.078480	7809.652007	14.435904	-0.061312	4.761635
307.585710	7801.508514	14.440909	-0.061401	4.759180
306.952134	7793.641557	14.445914	-0.061278	4.756810
307.198162	7785.558988	14.450919	-0.061319	4.754371
306.858746	7777.571198	14.455923	-0.061250	4.751961
306.810157	7769.560800	14.460928	-0.061236	4.749543
306.454438	7761.582267	14.465933	-0.061165	4.747133
306.535035	7753.459181	14.470938	-0.061174	4.744678
306.763774	7745.555959	14.475943	-0.061212	4.742287
306.471570	7737.522197	14.480947	-0.061152	4.739857
306.260039	7729.545775	14.485952	-0.061107	4.737443
306.350108	7721.508399	14.490957	-0.061119	4.735008
306.542663	7713.471627	14.495962	-0.061149	4.732572
306.776650	7705.483435	14.500967	-0.061188	4.730150
306.308636	7697.485014	14.505971	-0.061095	4.727725
305.987775	7689.540020	14.510976	-0.061030	4.725314
306.044839	7681.583718	14.515981	-0.061036	4.722898
306.222152	7673.485174	14.520986	-0.061063	4.720437
306.423298	7665.568545	14.525991	-0.061096	4.718030
306.102744	7657.573406	14.530995	-0.061031	4.715599
306.127647	7649.464054	14.536000	-0.061030	4.713131
306.091133	7641.544247	14.541005	-0.061018	4.710720
306.164981	7633.485513	14.546010	-0.061026	4.708265
305.898018	7625.583258	14.551015	-0.060972	4.705857
305.598535	7617.563231	14.556019	-0.060911	4.703412
305.581430	7609.577131	14.561024	-0.060902	4.700976
305.626656	7601.529951	14.566029	-0.060905	4.698520
305.652375	7593.509393	14.571034	-0.060905	4.696070
305.598374	7585.563267	14.576039	-0.060890	4.693642
305.500920	7577.517030	14.581043	-0.060866	4.691182
305.553212	7569.464213	14.586048	-0.060871	4.688719
305.339841	7561.572054	14.591053	-0.060826	4.686304
304.997490	7553.531900	14.596058	-0.060757	4.683842
305.304931	7545.605367	14.601063	-0.060809	4.681413
305.546827	7537.476018	14.606067	-0.060848	4.678921
304.999949	7529.636681	14.611072	-0.060741	4.676518
304.609270	7521.549548	14.616077	-0.060663	4.674036
304.497732	7513.470245	14.621082	-0.060637	4.671556
304.674731	7505.461611	14.626087	-0.060665	4.669096
304.755816	7497.445892	14.631091	-0.060675	4.666632
304.757179	7489.385617	14.636096	-0.060670	4.664153
304.465096	7481.556761	14.641101	-0.060610	4.661745
304.656595	7473.447249	14.646106	-0.060641	4.659248
304.525359	7465.546724	14.651111	-0.060611	4.656815
304.402371	7457.490352	14.656115	-0.060583	4.654333
304.147242	7449.552779	14.661120	-0.060530	4.651885
304.261510	7441.435132	14.666125	-0.060546	4.649381
304.190146	7433.494887	14.671130	-0.060527	4.646930
304.361494	7425.446446	14.676135	-0.060554	4.644445
304.582354	7417.473918	14.681139	-0.060590	4.641982
304.300390	7409.448677	14.686144	-0.060532	4.639501
304.369481	7401.498948	14.691149	-0.060540	4.637042
303.967377	7393.427163	14.696154	-0.060460	4.634543
303.946399	7385.507331	14.701159	-0.060451	4.632091
303.766870	7377.429849	14.706163	-0.060412	4.629589
304.398818	7369.372043	14.711168	-0.060524	4.627091
304.087047	7361.412306	14.716173	-0.060461	4.624622
304.347217	7353.421201	14.721178	-0.060504	4.622143
303.961619	7345.476377	14.726183	-0.060427	4.619676
304.325997	7337.450239	14.731187	-0.060490	4.617183
304.178254	7329.422958	14.736192	-0.060457	4.614688
304.076842	7321.482223	14.741197	-0.060433	4.612218
303.996937	7313.377187	14.746202	-0.060413	4.609696
304.177876	7305.500191	14.751207	-0.060441	4.607244
303.815049	7297.382035	14.756211	-0.060368	4.604715
303.549613	7289.477383	14.761216	-0.060314	4.602251
303.643904	7281.431339	14.766221	-0.060326	4.599742
303.397946	7273.448260	14.771226	-0.060275	4.597251
303.391161	7265.470454	14.776231	-0.060268	4.594761
303.123808	7257.402365	14.781235	-0.060213	4.592241
303.516551	7249.296414	14.786240	-0.060281	4.589708
303.679725	7241.367727	14.791245	-0.060306	4.587229
303.520583	7233.356290	14.796250	-0.060271	4.584723
303.661679	7225.433312	14.801255	-0.060292	4.582243
303.523042	7217.386702	14.806259	-0.060261	4.579722
303.036939	7209.444346	14.811264	-0.060166	4.577233
303.462642	7201.367291	14.816269	-0.060240	4.574701
303.116962	7193.395140	14.821274	-0.060170	4.572199
302.897747	7185.398797	14.826279	-0.060124	4.569689
303.146788	7177.346035	14.831283	-0.060165	4.567160
303.537255	7169.253920	14.836288	-0.060232	4.564618
303.301688	7161.430867	14.841293	-0.060183	4.562158
303.124075	7153.382503	14.846298	-0.060145	4.559626
302.946736	7145.442806	14.851303	-0.060107	4.557127
303.065367	7137.328783	14.856307	-0.060124	4.554571
303.177171	7129.368897	14.861312	-0.060139	4.552064
303.377221	7121.308682	14.866317	-0.060171	4.549523
303.178259	7113.296865	14.871322	-0.060129	4.546995
303.361994	7105.309987	14.876327	-0.060158	4.544475
303.172010	7097.390105	14.881331	-0.060117	4.541973
303.427969	7089.314543	14.886336	-0.060160	4.539422
303.376770	7081.316375	14.891341	-0.060145	4.536893
303.586930	7073.294562	14.896346	-0.060179	4.534356
303.178849	7065.388664	14.901351	-0.060097	4.531853
303.232199	7057.318158	14.906355	-0.060102	4.529297
303.223661	7049.376927	14.911360	-0.060095	4.526781
303.562677	7041.283967	14.916365	-0.060153	4.524216
302.971363	7033.400994	14.921370	-0.060038	4.521713
303.086638	7025.325315	14.926375	-0.060054	4.519150
302.838867	7017.388826	14.931379	-0.060003	4.516629
302.628397	7009.356277	14.936384	-0.059958	4.514076
302.849357	7001.340205	14.941389	-0.059994	4.511528
302.428182	6993.305507	14.946394	-0.059910	4.508971
302.593462	6985.299123	14.951399	-0.059936	4.506423
302.332127	6977.270891	14.956403	-0.059882	4.503865
302.179591	6969.333194	14.961408	-0.059848	4.501335
302.077161	6961.316213	14.966413	-0.059824	4.498778
301.883717	6953.314749	14.971418	-0.059783	4.496225
301.745940	6945.299615	14.976423	-0.059752	4.493666
302.047475	6937.263948	14.981427	-0.059803	4.491100
301.707271	6929.261602	14.986432	-0.059734	4.488541
301.655730	6921.323602	14.991437	-0.059719	4.486003
301.911895	6913.241635	14.996442	-0.059762	4.483418
302.054821	6905.297390	15.001447	-0.059783	4.480876
301.492547	6897.283508	15.006451	-0.059673	4.478306
301.599622	6889.282647	15.011456	-0.059688	4.475742
302.142949	6881.267516	15.016461	-0.059784	4.473175
301.636143	6873.244598	15.021466	-0.059684	4.470598
301.387440	6865.259706	15.026471	-0.059632	4.468033
301.294645	6857.259722	15.031475	-0.059610	4.465463
301.300082	6849.262923	15.036480	-0.059606	4.462893
301.040940	6841.311613	15.041485	-0.059552	4.460334
300.872839	6833.285021	15.046490	-0.059516	4.457750
300.705731	6825.303854	15.051495	-0.059479	4.455180
300.472446	6817.308063	15.056499	-0.059431	4.452602
300.597961	6809.188340	15.061504	-0.059449	4.449986
300.644052	6801.260413	15.066509	-0.059452	4.447429
300.385775	6793.249151	15.071514	-0.059399	4.444842
300.385637	6785.333129	15.076519	-0.059393	4.442286
300.474295	6777.204787	15.081523	-0.059405	4.439660
300.443283	6769.255080	15.086528	-0.059394	4.437089
300.609695	6761.194715	15.091533	-0.059419	4.434483
300.246670	6753.237837	15.096538	-0.059346	4.431905
300.383382	6745.220168	15.101543	-0.059367	4.429309
300.277725	6737.196981	15.106547	-0.059342	4.426709
300.279422	6729.153543	15.111552	-0.059337	4.424100
300.378639	6721.279521	15.116557	-0.059350	4.421546
300.131676	6713.201927	15.121562	-0.059299	4.418923
300.292540	6705.244716	15.126567	-0.059323	4.416339
300.179335	6697.192535	15.131571	-0.059297	4.413721
300.017753	6689.196958	15.136576	-0.059262	4.411120
299.904680	6681.219636	15.141581	-0.059235	4.408523
300.191463	6673.139704	15.146586	-0.059284	4.405894
299.967657	6665.257361	15.151591	-0.059237	4.403325
299.818710	6657.237508	15.156595	-0.059204	4.400709
299.810573	6649.234059	15.161600	-0.059197	4.398099
300.303809	6641.189029	15.166605	-0.059284	4.395476
299.807005	6633.257443	15.171610	-0.059186	4.392883
299.726045	6625.251606	15.176615	-0.059165	4.390266
299.590121	6617.290849	15.181619	-0.059135	4.387663
299.540969	6609.276795	15.186624	-0.059121	4.385040
299.606145	6601.300446	15.191629	-0.059127	4.382430
299.042209	6593.304958	15.196634	-0.059017	4.379807
299.362288	6585.323266	15.201639	-0.059072	4.377193
299.620861	6577.234292	15.206643	-0.059114	4.374542
299.360358	6569.320230	15.211648	-0.059061	4.371944
299.485656	6561.232386	15.216653	-0.059079	4.369289
299.275186	6553.305031	15.221658	-0.059034	4.366683
299.118634	6545.339524	15.226663	-0.059000	4.364063
298.944755	6537.399185	15.231667	-0.058962	4.361450
299.096474	6529.330182	15.236672	-0.058985	4.358796
299.467743	6521.326414	15.241677	-0.059049	4.356163
299.129840	6513.287814	15.246682	-0.058981	4.353511
299.091475	6505.275687	15.251687	-0.058969	4.350869
298.910749	6497.248139	15.256691	-0.058930	4.348219
298.959481	6489.187053	15.261696	-0.058933	4.345558
298.887610	6481.294385	15.266701	-0.058915	4.342950
298.725242	6473.261367	15.271706	-0.058879	4.340294
298.451535	6465.332289	15.276711	-0.058823	4.337669
298.520964	6457.226226	15.281715	-0.058831	4.334987
298.644725	6449.263311	15.286720	-0.058849	4.332351
298.677032	6441.306527	15.291725	-0.058849	4.329715
298.448913	6433.294258	15.296730	-0.058802	4.327056
298.568787	6425.229327	15.301735	-0.058819	4.324382
298.254607	6417.366518	15.306739	-0.058755	4.321769
298.163289	6409.266119	15.311744	-0.058733	4.319078
298.314181	6401.321387	15.316749	-0.058756	4.316438
298.425825	6393.220131	15.321754	-0.058771	4.313745
298.415292	6385.264958	15.326759	-0.058764	4.311097
298.201727	6377.256298	15.331763	-0.058719	4.308429
298.086370	6369.242595	15.336768	-0.058692	4.305758
298.185724	6361.246900	15.341773	-0.058705	4.303093
297.848726	6353.294072	15.346778	-0.058637	4.300436
297.968993	6345.311459	15.351783	-0.058654	4.297773
297.831754	6337.269779	15.356787	-0.058624	4.295085
297.686463	6329.215676	15.361792	-0.058591	4.292392
297.939529	6321.225645	15.366797	-0.058633	4.289722
298.152415	6313.203379	15.371802	-0.058668	4.287039
298.216983	6305.176243	15.376807	-0.058674	4.284352
298.130500	6297.258993	15.381811	-0.058653	4.281698
297.949062	6289.247936	15.386816	-0.058614	4.279010
298.186371	6281.306268	15.391821	-0.058653	4.276348
297.665623	6273.269551	15.396826	-0.058551	4.273645
297.804313	6265.225477	15.401831	-0.058571	4.270944
297.528978	6257.237554	15.406835	-0.058515	4.268257
297.679642	6249.185633	15.411840	-0.058537	4.265550
297.819712	6241.218834	15.416845	-0.058558	4.262870
297.346759	6233.224316	15.421850	-0.058465	4.260173
297.263480	6225.297449	15.426855	-0.058444	4.257501
297.178411	6217.208130	15.431859	-0.058423	4.254772
297.112125	6209.253889	15.436864	-0.058406	4.252087
297.237780	6201.191604	15.441869	-0.058424	4.249367
296.752824	6193.280732	15.446874	-0.058328	4.246689
296.916735	6185.209075	15.451879	-0.058353	4.243962
297.081505	6177.258767	15.456883	-0.058379	4.241274
296.843519	6169.213596	15.461888	-0.058329	4.238548
296.677815	6161.258036	15.466893	-0.058293	4.235852
296.604411	6153.204314	15.471898	-0.058274	4.233121
296.812651	6145.237004	15.476903	-0.058308	4.230421
296.768405	6137.183503	15.481907	-0.058294	4.227688
296.732936	6129.159768	15.486912	-0.058282	4.224963
296.947615	6121.224016	15.491917	-0.058317	4.222268
296.771754	6113.183961	15.496922	-0.058279	4.219532
296.857777	6105.254315	15.501927	-0.058290	4.216835
296.620100	6097.225855	15.506931	-0.058240	4.214099
296.569636	6089.249608	15.511936	-0.058226	4.211381
296.539570	6081.201870	15.516941	-0.058215	4.208637
296.457528	6073.213300	15.521946	-0.058194	4.205911
296.384352	6065.251594	15.526951	-0.058175	4.203193
296.187899	6057.249027	15.531955	-0.058134	4.200457
296.253077	6049.264704	15.536960	-0.058141	4.197728
296.291903	6041.241750	15.541965	-0.058143	4.194985
295.643268	6033.238759	15.546970	-0.058016	4.192238
295.744426	6025.214226	15.551975	-0.058030	4.189491
295.758442	6017.154266	15.556979	-0.058027	4.186729
295.547759	6009.197649	15.561984	-0.057983	4.183998
295.613994	6001.225589	15.566989	-0.057990	4.181263
295.860830	5993.166850	15.571994	-0.058031	4.178499
295.698382	5985.231566	15.576999	-0.057995	4.175770
295.561104	5977.216221	15.582003	-0.057964	4.173012
295.364402	5969.224718	15.587008	-0.057923	4.170260
295.466804	5961.204115	15.592013	-0.057936	4.167500
295.517550	5953.158978	15.597018	-0.057940	4.164729
295.371301	5945.258605	15.602023	-0.057908	4.162004
295.091885	5937.261649	15.607027	-0.057851	4.159241
295.302372	5929.280835	15.612032	-0.057885	4.156489
295.355561	5921.241542	15.617037	-0.057889	4.153713
295.299335	5913.219848	15.622042	-0.057874	4.150939
295.302438	5905.298751	15.627047	-0.057869	4.148199
294.974207	5897.273749	15.632051	-0.057803	4.145417
294.788964	5889.309191	15.637056	-0.057763	4.142656
295.016082	5881.225253	15.642061	-0.057800	4.139857
294.688656	5873.269759	15.647066	-0.057734	4.137093
294.918653	5865.209099	15.652071	-0.057771	4.134299
295.010131	5857.225695	15.657075	-0.057783	4.131528
294.852092	5849.235830	15.662080	-0.057748	4.128749
294.708567	5841.253538	15.667085	-0.057716	4.125971
294.608161	5833.249873	15.672090	-0.057692	4.123184
294.477443	5825.276175	15.677095	-0.057663	4.120405
294.435343	5817.275720	15.682099	-0.057650	4.117617
294.467220	5809.209724	15.687104	-0.057650	4.114805
294.720518	5801.258372	15.692109	-0.057692	4.112033
294.399666	5793.168396	15.697114	-0.057627	4.109204
294.776101	5785.193309	15.702119	-0.057692	4.106423
294.625336	5777.198614	15.707123	-0.057659	4.103625
294.732645	5769.235412	15.712128	-0.057674	4.100840
294.420751	5761.273488	15.717133	-0.057610	4.098048
294.340617	5753.226465	15.722138	-0.057590	4.095227
294.526442	5745.293222	15.727143	-0.057619	4.092448
294.364147	5737.179729	15.732147	-0.057584	4.089599
294.247375	5729.218493	15.737152	-0.057557	4.086802
294.568288	5721.185654	15.742157	-0.057611	4.083984
294.507319	5713.254322	15.747162	-0.057595	4.081195
294.337881	5705.235493	15.752167	-0.057558	4.078371
293.875632	5697.303974	15.757171	-0.057467	4.075572
294.176600	5689.243413	15.762176	-0.057517	4.072736
293.899009	5681.248748	15.767181	-0.057461	4.069913
293.629771	5673.262930	15.772186	-0.057405	4.067092
294.202251	5665.174483	15.777191	-0.057506	4.064245
294.064694	5657.283327	15.782195	-0.057476	4.061455
293.836483	5649.237457	15.787200	-0.057428	4.058606
293.990356	5641.264261	15.792205	-0.057451	4.055788
293.762345	5633.235921	15.797210	-0.057404	4.052942
293.619201	5625.272083	15.802215	-0.057372	4.050118
293.186329	5617.308347	15.807219	-0.057286	4.047288
293.299480	5609.270414	15.812224	-0.057302	4.044437
293.702295	5601.288319	15.817229	-0.057371	4.041610
293.137311	5593.315115	15.822234	-0.057261	4.038768
293.567042	5585.284928	15.827239	-0.057336	4.035920
293.123461	5577.304548	15.832243	-0.057248	4.033073
292.847406	5569.282862	15.837248	-0.057191	4.030212
293.004734	5561.235626	15.842253	-0.057215	4.027348
292.953701	5553.212457	15.847258	-0.057200	4.024486
292.793529	5545.300682	15.852263	-0.057165	4.021660
292.914374	5537.250317	15.857267	-0.057183	4.018788
292.843594	5529.277533	15.862272	-0.057164	4.015938
292.978771	5521.286787	15.867277	-0.057184	4.013083
292.831419	5513.260086	15.872282	-0.057151	4.010208
293.080902	5505.268310	15.877287	-0.057193	4.007350
292.954727	5497.224269	15.882291	-0.057164	4.004465
292.609210	5489.354971	15.887296	-0.057094	4.001638
292.832455	5481.322309	15.892301	-0.057131	3.998759
292.903061	5473.291410	15.897306	-0.057139	3.995876
293.051658	5465.313744	15.902311	-0.057161	3.993011
292.820547	5457.302934	15.907315	-0.057113	3.990126
292.819630	5449.287653	15.912320	-0.057107	3.987242
292.611022	5441.299624	15.917325	-0.057063	3.984361
292.239410	5433.341073	15.922330	-0.056989	3.981486
292.188505	5425.356154	15.927335	-0.056974	3.978605
292.305272	5417.288322	15.932339	-0.056990	3.975695
292.019806	5409.335370	15.937344	-0.056932	3.972817
291.827950	5401.329239	15.942349	-0.056891	3.969920
292.053416	5393.283084	15.947354	-0.056928	3.967013
292.184294	5385.263019	15.952359	-0.056947	3.964112
291.950914	5377.324050	15.957363	-0.056898	3.961232
292.187278	5369.293090	15.962368	-0.056937	3.958324
291.987051	5361.335768	15.967373	-0.056894	3.955434
292.064628	5353.289350	15.972378	-0.056904	3.952514
292.015048	5345.285442	15.977383	-0.056889	3.949605
291.905074	5337.350652	15.982387	-0.056863	3.946717
292.014412	5329.256857	15.987392	-0.056878	3.943774
291.862822	5321.355729	15.992397	-0.056845	3.940894
291.876340	5313.310539	15.997402	-0.056842	3.937963
292.031544	5305.293883	16.002407	-0.056866	3.935042
291.707723	5297.333919	16.007411	-0.056800	3.932131
291.578569	5289.309925	16.012416	-0.056771	3.929198
291.335344	5281.362054	16.017421	-0.056721	3.926288
291.332601	5273.292240	16.022426	-0.056715	3.923336
291.679398	5265.319016	16.027431	-0.056774	3.920424
291.430773	5257.394481	16.032435	-0.056723	3.917516
291.420372	5249.319294	16.037440	-0.056715	3.914556
291.256936	5241.389467	16.042445	-0.056680	3.911643
291.216340	5233.348483	16.047450	-0.056667	3.908690
291.328841	5225.376644	16.052455	-0.056683	3.905763
291.090784	5217.404357	16.057459	-0.056633	3.902827
291.045679	5209.371666	16.062464	-0.056619	3.899870
291.027115	5201.413128	16.067469	-0.056611	3.896939
291.336214	5193.327405	16.072474	-0.056663	3.893965
291.330885	5185.375089	16.077479	-0.056657	3.891032
291.219949	5177.393198	16.082483	-0.056631	3.888084
290.865375	5169.387027	16.087488	-0.056560	3.885119
290.722880	5161.462250	16.092493	-0.056528	3.882187
290.730828	5153.399293	16.097498	-0.056524	3.879204
291.121512	5145.380046	16.102503	-0.056591	3.876243
290.732372	5137.354287	16.107507	-0.056514	3.873261
290.210642	5129.321344	16.112512	-0.056411	3.870272
290.844302	5121.305793	16.117517	-0.056524	3.867310
290.768844	5113.262550	16.122522	-0.056505	3.864322
290.685301	5105.433431	16.127527	-0.056484	3.861410
290.739185	5097.367449	16.132531	-0.056489	3.858411
290.643502	5089.384234	16.137536	-0.056466	3.855437
290.689677	5081.417469	16.142541	-0.056469	3.852470
290.478190	5073.376322	16.147546	-0.056424	3.849468
290.473437	5065.424050	16.152551	-0.056418	3.846501
290.477288	5057.371277	16.157555	-0.056414	3.843494
290.333998	5049.389371	16.162560	-0.056382	3.840508
290.915855	5041.383703	16.167565	-0.056485	3.837527
290.396402	5033.411332	16.172570	-0.056383	3.834532
289.862522	5025.533757	16.177575	-0.056278	3.831569
289.799982	5017.474734	16.182579	-0.056261	3.828547
289.980301	5009.356093	16.187584	-0.056290	3.825505
289.905034	5001.445272	16.192589	-0.056270	3.822533
289.865225	4993.381547	16.197594	-0.056258	3.819502
289.894055	4985.475314	16.202599	-0.056258	3.816530
289.720232	4977.406667	16.207603	-0.056220	3.813489
289.496470	4969.429584	16.212608	-0.056173	3.810480
289.917370	4961.414858	16.217613	-0.056246	3.807468
289.641699	4953.425497	16.222618	-0.056190	3.804448
289.509361	4945.533054	16.227623	-0.056160	3.801465
289.461455	4937.477337	16.232627	-0.056146	3.798420
289.601660	4929.449570	16.237632	-0.056167	3.795388
289.431137	4921.500902	16.242637	-0.056130	3.792376
289.427147	4913.428042	16.247642	-0.056124	3.789318
289.609216	4905.453087	16.252647	-0.056152	3.786300
289.163059	4897.460133	16.257651	-0.056064	3.783257
289.301527	4889.479272	16.262656	-0.056085	3.780230
288.929547	4881.581032	16.267661	-0.056010	3.777220
288.829887	4873.513782	16.272666	-0.055986	3.774150
288.965803	4865.513756	16.277671	-0.056006	3.771109
289.201873	4857.469565	16.282675	-0.056045	3.768050
289.469858	4849.446159	16.287680	-0.056090	3.764998
289.200564	4841.543442	16.292685	-0.056034	3.761977
289.112337	4833.510609	16.297690	-0.056013	3.758907
289.448851	4825.534004	16.302695	-0.056070	3.755868
289.040887	4817.542077	16.307699	-0.055989	3.752801
288.837002	4809.551901	16.312704	-0.055946	3.749738
289.111976	4801.515472	16.317709	-0.055991	3.746666
288.727335	4793.551792	16.322714	-0.055915	3.743603
288.934057	4785.553998	16.327719	-0.055948	3.740540
288.895888	4777.560728	16.332723	-0.055936	3.737469
288.516028	4769.555752	16.337728	-0.055860	3.734383
288.480044	4761.589414	16.342733	-0.055848	3.731318
288.102099	4753.591298	16.347738	-0.055772	3.728229
288.238623	4745.582306	16.352743	-0.055792	3.725147
288.035312	4737.637940	16.357747	-0.055749	3.722078
288.089482	4729.565110	16.362752	-0.055754	3.718964
287.848936	4721.689884	16.367757	-0.055704	3.715916
287.756164	4713.593424	16.372762	-0.055681	3.712784
287.753419	4705.531706	16.377767	-0.055675	3.709665
287.702939	4697.552505	16.382771	-0.055661	3.706574
287.990425	4689.504132	16.387776	-0.055709	3.703462
288.054792	4681.541803	16.392781	-0.055716	3.700375
287.735306	4673.600786	16.397786	-0.055651	3.697284
287.845071	4665.579631	16.402791	-0.055666	3.694171
288.033687	4657.590332	16.407795	-0.055696	3.691069
287.560317	4649.565396	16.412800	-0.055603	3.687933
287.344050	4641.617253	16.417805	-0.055557	3.684831
287.292706	4633.660595	16.422810	-0.055543	3.681728
287.491516	4625.625493	16.427815	-0.055574	3.678598
287.246766	4617.671679	16.432819	-0.055523	3.675486
287.411625	4609.650887	16.437824	-0.055549	3.672355
287.097321	4601.681256	16.442829	-0.055485	3.669229
287.116556	4593.641970	16.447834	-0.055483	3.666082
287.156035	4585.664717	16.452839	-0.055486	3.662957
286.990149	4577.686337	16.457843	-0.055449	3.659824
286.853189	4569.707277	16.462848	-0.055419	3.656688
286.927168	4561.693292	16.467853	-0.055427	3.653542
286.729338	4553.695026	16.472858	-0.055385	3.650391
287.116357	4545.667178	16.477863	-0.055452	3.647243
287.091605	4537.657849	16.482867	-0.055442	3.644087
286.817846	4529.743624	16.487872	-0.055386	3.640960
286.904012	4521.758478	16.492877	-0.055397	3.637812
286.586258	4513.734003	16.497882	-0.055332	3.634634
286.463187	4505.791173	16.502887	-0.055304	3.631491
286.540091	4497.705232	16.507891	-0.055313	3.628294
286.613037	4489.664505	16.512896	-0.055321	3.625112
286.473271	4481.746181	16.517901	-0.055290	3.621971
286.460765	4473.688682	16.522906	-0.055283	3.618774
286.669369	4465.722087	16.527911	-0.055316	3.615618
286.788741	4457.710741	16.532915	-0.055333	3.612438
286.527805	4449.710624	16.537920	-0.055279	3.609249
286.216331	4441.838216	16.542925	-0.055216	3.606106
286.331933	4433.751129	16.547930	-0.055232	3.602888
286.503795	4425.750820	16.552935	-0.055259	3.599703
286.458723	4417.798547	16.557939	-0.055245	3.596527
286.244629	4409.775984	16.562944	-0.055200	3.593316
286.198972	4401.841085	16.567949	-0.055187	3.590143
286.217099	4393.789173	16.572954	-0.055185	3.586921
286.150724	4385.800655	16.577959	-0.055167	3.583719
286.325720	4377.780254	16.582963	-0.055194	3.580509
286.593596	4369.773233	16.587968	-0.055239	3.577305
286.235585	4361.835834	16.592973	-0.055167	3.574106
286.113087	4353.841389	16.597978	-0.055139	3.570889
286.015263	4345.848469	16.602983	-0.055116	3.567670
286.068258	4337.811873	16.607987	-0.055120	3.564435
286.003141	4329.868166	16.612992	-0.055103	3.561232
285.922529	4321.935142	16.617997	-0.055083	3.558029
285.948053	4313.872919	16.623002	-0.055082	3.554774
285.980634	4305.853050	16.628007	-0.055083	3.551534
285.618647	4297.869203	16.633011	-0.055010	3.548293
285.617439	4289.839655	16.638016	-0.055005	3.545042
285.597913	4281.916679	16.643021	-0.054996	3.541830
285.542433	4273.869056	16.648026	-0.054980	3.538564
285.706808	4265.829544	16.653031	-0.055006	3.535305
285.282960	4257.952084	16.658035	-0.054922	3.532090
285.344734	4249.899969	16.663040	-0.054928	3.528816
285.016284	4241.952433	16.668045	-0.054861	3.525570
285.148535	4233.951831	16.673050	-0.054881	3.522314
285.061174	4225.918417	16.678055	-0.054859	3.519034
285.318747	4217.935738	16.683059	-0.054902	3.515783
285.277976	4209.907481	16.688064	-0.054889	3.512501
285.443909	4201.901700	16.693069	-0.054915	3.509232
285.344529	4193.934228	16.698074	-0.054891	3.505967
284.860418	4186.006295	16.703079	-0.054796	3.502702
284.972034	4177.965542	16.708083	-0.054811	3.499407
284.777587	4170.025893	16.713088	-0.054770	3.496141
284.639744	4162.044432	16.718093	-0.054739	3.492856
284.518958	4154.017597	16.723098	-0.054711	3.489550
284.644430	4146.022598	16.728103	-0.054729	3.486263
284.764420	4138.014330	16.733107	-0.054746	3.482966
284.635263	4129.998913	16.738112	-0.054717	3.479655
284.561561	4122.075120	16.743117	-0.054698	3.476381
284.410632	4114.045052	16.748122	-0.054665	3.473057
284.235821	4106.086539	16.753127	-0.054627	3.469759
284.736203	4097.960828	16.758131	-0.054715	3.466410
284.881460	4089.949296	16.763136	-0.054736	3.463095
284.731744	4082.066557	16.768141	-0.054703	3.459819
284.796200	4074.041528	16.773146	-0.054710	3.456488
284.825104	4066.069172	16.778151	-0.054710	3.453175
284.325963	4058.154010	16.783155	-0.054612	3.449865
284.397102	4050.105885	16.788160	-0.054620	3.446515
284.038111	4042.194011	16.793165	-0.054548	3.443204
284.298727	4034.127786	16.798170	-0.054591	3.439847
283.981082	4026.192163	16.803175	-0.054527	3.436521
284.166826	4018.155203	16.808179	-0.054556	3.433167
284.425965	4010.084088	16.813184	-0.054599	3.429798
284.234742	4002.166544	16.818189	-0.054558	3.426475
284.416441	3994.102662	16.823194	-0.054587	3.423100
284.150347	3986.198846	16.828199	-0.054532	3.419772
283.470885	3978.320662	16.833203	-0.054401	3.416438
283.638073	3970.226026	16.838208	-0.054426	3.413040
283.564815	3962.242780	16.843213	-0.054407	3.409676
283.322412	3954.254430	16.848218	-0.054357	3.406301
283.513349	3946.208354	16.853223	-0.054387	3.402913
283.303832	3938.255384	16.858227	-0.054343	3.399547
283.557048	3930.237576	16.863232	-0.054385	3.396168
283.134368	3922.273803	16.868237	-0.054301	3.392783
282.943313	3914.240804	16.873242	-0.054260	3.389373
283.302324	3906.206129	16.878247	-0.054322	3.385980
283.463457	3898.209665	16.883251	-0.054347	3.382592
283.303399	3890.212944	16.888256	-0.054311	3.379190
283.605814	3882.232677	16.893261	-0.054363	3.375807
282.825408	3874.347797	16.898266	-0.054212	3.372422
282.770091	3866.313569	16.903271	-0.054196	3.368996
282.881845	3858.315388	16.908275	-0.054212	3.365589
282.367264	3850.418068	16.913280	-0.054111	3.362198
282.607095	3842.362051	16.918285	-0.054150	3.358764
282.366482	3834.379001	16.923290	-0.054100	3.355339
282.499380	3826.388076	16.928295	-0.054120	3.351922
282.277420	3818.397265	16.933299	-0.054073	3.348488
282.348340	3810.351767	16.938304	-0.054081	3.345038
282.718089	3802.378112	16.943309	-0.054145	3.341626
282.990099	3794.327510	16.948314	-0.054190	3.338175
282.987464	3786.346533	16.953319	-0.054184	3.334739
282.790193	3778.435328	16.958323	-0.054143	3.331322
282.445621	3770.460878	16.963328	-0.054073	3.327869
282.534160	3762.448829	16.968333	-0.054084	3.324412
282.041336	3754.525446	16.973338	-0.053987	3.320968
282.203008	3746.494641	16.978343	-0.054012	3.317499
282.264982	3738.467469	16.983347	-0.054018	3.314025
281.745075	3730.520004	16.988352	-0.053916	3.310558
281.842190	3722.497902	16.993357	-0.053929	3.307079
281.708150	3714.500158	16.998362	-0.053899	3.303599
281.529766	3706.552247	17.003367	-0.053861	3.300134
281.329671	3698.594688	17.008371	-0.053818	3.296661
281.385367	3690.549948	17.013376	-0.053823	3.293156
281.543022	3682.521574	17.018381	-0.053847	3.289659
281.501375	3674.526382	17.023386	-0.053834	3.286164
281.454678	3666.589414	17.028391	-0.053820	3.282692
281.386079	3658.592329	17.033395	-0.053802	3.279188
281.351201	3650.594306	17.038400	-0.053791	3.275681
281.378980	3642.628941	17.043405	-0.053791	3.272188
281.318971	3634.610589	17.048410	-0.053774	3.268663
281.517554	3626.595342	17.053415	-0.053806	3.265147
281.326155	3618.653304	17.058419	-0.053765	3.261644
280.898989	3610.728438	17.063424	-0.053680	3.258134
281.200449	3602.691852	17.068429	-0.053731	3.254602
281.010318	3594.694359	17.073434	-0.053690	3.251063
280.883864	3586.730046	17.078439	-0.053662	3.247537
280.756565	3578.730107	17.083443	-0.053633	3.243991
280.558547	3570.770297	17.088448	-0.053591	3.240456
280.678279	3562.775891	17.093453	-0.053608	3.236915
280.775596	3554.703750	17.098458	-0.053620	3.233335
280.598704	3546.740925	17.103463	-0.053582	3.229789
280.508167	3538.761900	17.108467	-0.053560	3.226234
280.429979	3530.757620	17.113472	-0.053540	3.222665
280.607647	3522.752525	17.118477	-0.053568	3.219103
280.790698	3514.743812	17.123482	-0.053597	3.215535
280.574041	3506.780106	17.128487	-0.053551	3.211966
280.526290	3498.814722	17.133491	-0.053537	3.208400
280.426943	3490.792835	17.138496	-0.053514	3.204802
280.555499	3482.829703	17.143501	-0.053532	3.201236
280.523509	3474.845020	17.148506	-0.053521	3.197650
280.442687	3466.874734	17.153511	-0.053501	3.194064
280.115528	3458.932477	17.158515	-0.053435	3.190476
280.151177	3450.889261	17.163520	-0.053436	3.186854
280.352150	3442.887508	17.168525	-0.053468	3.183254
280.184276	3434.878173	17.173530	-0.053432	3.179630
279.783714	3427.002269	17.178535	-0.053352	3.176053
279.735401	3418.995450	17.183539	-0.053338	3.172427
279.828589	3410.942603	17.188544	-0.053350	3.168783
280.264366	3402.921699	17.193549	-0.053426	3.165164
280.129958	3394.954248	17.198554	-0.053395	3.161540
279.926328	3387.026170	17.203559	-0.053352	3.157927
279.764043	3379.051766	17.208563	-0.053317	3.154290
279.792026	3371.028073	17.213568	-0.053317	3.150635
279.928170	3363.030297	17.218573	-0.053337	3.146992
279.421583	3355.072184	17.223578	-0.053237	3.143335
279.194614	3347.120284	17.228583	-0.053190	3.139688
279.202008	3339.155695	17.233587	-0.053186	3.136042
279.228999	3331.101057	17.238592	-0.053186	3.132352
279.149348	3323.118270	17.243597	-0.053166	3.128685
278.814161	3315.149500	17.248602	-0.053098	3.125009
279.070317	3307.152470	17.253607	-0.053140	3.121342
279.235931	3299.155546	17.258611	-0.053166	3.117667
279.209374	3291.145426	17.263616	-0.053156	3.113973
279.191347	3283.190605	17.268621	-0.053147	3.110300
279.109860	3275.208418	17.273626	-0.053127	3.106607
278.813424	3267.253561	17.278631	-0.053066	3.102913
278.844783	3259.253407	17.283635	-0.053067	3.099208
278.697072	3251.284433	17.288640	-0.053034	3.095505
278.691561	3243.301805	17.293645	-0.053028	3.091798
278.436256	3235.294603	17.298650	-0.052975	3.088063
278.597729	3227.245754	17.303655	-0.053000	3.084324
278.298134	3219.392554	17.308659	-0.052939	3.080650
278.301923	3211.365179	17.313664	-0.052934	3.076905
278.673121	3203.291646	17.318669	-0.052998	3.073151
278.156036	3195.308921	17.323674	-0.052897	3.069392
278.053436	3187.347955	17.328679	-0.052872	3.065659
278.045267	3179.376299	17.333683	-0.052866	3.061920
278.225862	3171.350904	17.338688	-0.052894	3.058161
278.297747	3163.373818	17.343693	-0.052902	3.054415
277.995031	3155.424346	17.348698	-0.052841	3.050659
278.072425	3147.437814	17.353703	-0.052850	3.046900
278.369481	3139.409665	17.358707	-0.052900	3.043127
278.026190	3131.488213	17.363712	-0.052831	3.039368
277.899109	3123.553358	17.368717	-0.052802	3.035609
277.799583	3115.545117	17.373722	-0.052778	3.031811
277.585894	3107.564268	17.378727	-0.052733	3.028017
277.909910	3099.497944	17.383731	-0.052788	3.024203
277.859045	3091.539073	17.388736	-0.052773	3.020418
277.947564	3083.547894	17.393741	-0.052784	3.016619
277.715157	3075.615236	17.398746	-0.052736	3.012827
277.909989	3067.564169	17.403751	-0.052767	3.008995
277.739239	3059.613178	17.408755	-0.052730	3.005188
277.857172	3051.631080	17.413760	-0.052747	3.001376
277.987103	3043.657128	17.418765	-0.052766	2.997563
277.235870	3035.775361	17.423770	-0.052621	2.993745
277.061686	3027.787491	17.428775	-0.052583	2.989900
277.193377	3019.759557	17.433779	-0.052602	2.986047
277.477942	3011.692389	17.438784	-0.052650	2.982178
277.677877	3003.710049	17.443789	-0.052682	2.978340
277.279761	2995.763804	17.448794	-0.052602	2.974484
277.513995	2987.757612	17.453799	-0.052641	2.970626
277.220079	2979.831282	17.458803	-0.052581	2.966775
276.923520	2971.866755	17.463808	-0.052520	2.962900
277.044628	2963.898166	17.468813	-0.052538	2.959040
276.825941	2955.923054	17.473818	-0.052492	2.955154
277.134255	2947.844496	17.478823	-0.052544	2.951240
277.336015	2939.834915	17.483827	-0.052576	2.947349
277.534753	2931.805435	17.488832	-0.052608	2.943443
277.483578	2923.897658	17.493837	-0.052593	2.939578
277.549584	2915.931267	17.498842	-0.052600	2.935686
277.344371	2907.998951	17.503847	-0.052557	2.931790
277.499503	2899.980213	17.508851	-0.052580	2.927866
277.085413	2892.069454	17.513856	-0.052498	2.923959
276.887403	2884.144898	17.518861	-0.052456	2.920052
276.625452	2876.165283	17.523866	-0.052402	2.916109
276.423814	2868.124713	17.528871	-0.052359	2.912134
276.542230	2860.072198	17.533875	-0.052376	2.908165
276.475292	2852.072133	17.538880	-0.052358	2.904206
276.583148	2844.117662	17.543885	-0.052373	2.900274
275.929949	2836.220793	17.548890	-0.052246	2.896323
276.274177	2828.158377	17.553895	-0.052305	2.892340
276.156698	2820.197073	17.558899	-0.052278	2.888376
275.906206	2812.207212	17.563904	-0.052226	2.884385
275.813755	2804.310861	17.568909	-0.052204	2.880444
275.668814	2796.343793	17.573914	-0.052172	2.876459
275.653087	2788.338265	17.578919	-0.052163	2.872457
275.650703	2780.338027	17.583923	-0.052158	2.868452
275.626989	2772.309061	17.588928	-0.052148	2.864426
275.841095	2764.357570	17.593933	-0.052183	2.860447
275.354272	2756.426150	17.598938	-0.052087	2.856433
275.190236	2748.450703	17.603943	-0.052051	2.852409
275.368639	2740.422685	17.608947	-0.052079	2.848372
274.803783	2732.480579	17.613952	-0.051969	2.844330
275.072766	2724.508708	17.618957	-0.052013	2.840316
275.173087	2716.498936	17.623962	-0.052027	2.836267
275.078956	2708.521086	17.628967	-0.052004	2.832217
274.711837	2700.581262	17.633971	-0.051930	2.828165
274.712744	2692.561419	17.638976	-0.051925	2.824088
274.990200	2684.571404	17.643981	-0.051972	2.820036
275.037992	2676.561820	17.648986	-0.051975	2.815955
274.911526	2668.608489	17.653991	-0.051947	2.811886
274.798602	2660.663333	17.658995	-0.051920	2.807817
274.646265	2652.661243	17.664000	-0.051887	2.803710
274.888635	2644.665671	17.669005	-0.051927	2.799624
274.426741	2636.790053	17.674010	-0.051836	2.795551
274.382016	2628.768770	17.679015	-0.051822	2.791423
274.338346	2620.775000	17.684019	-0.051809	2.787302
274.250686	2612.782517	17.689024	-0.051787	2.783174
274.233662	2604.840731	17.694029	-0.051779	2.779069
274.087067	2596.874701	17.699034	-0.051746	2.774939
274.193052	2588.863113	17.704039	-0.051761	2.770794
274.385708	2580.872443	17.709043	-0.051791	2.766658
273.964486	2572.963292	17.714048	-0.051708	2.762522
274.033821	2564.973885	17.719053	-0.051715	2.758367
274.059510	2556.977122	17.724058	-0.051715	2.754200
273.869655	2548.982839	17.729063	-0.051674	2.750014
273.924953	2540.976987	17.734067	-0.051679	2.745832
273.752012	2533.030798	17.739072	-0.051642	2.741659
273.892085	2525.055809	17.744077	-0.051663	2.737485
273.789680	2517.054238	17.749082	-0.051638	2.733276
273.645015	2509.090874	17.754087	-0.051606	2.729077
273.830235	2501.083636	17.759091	-0.051635	2.724869
273.582219	2493.172119	17.764096	-0.051584	2.720678
273.521876	2485.226704	17.769101	-0.051567	2.716475
273.453466	2477.250397	17.774106	-0.051550	2.712248
273.414384	2469.263598	17.779111	-0.051537	2.708011
273.312976	2461.313904	17.784115	-0.051513	2.703783
273.411056	2453.278016	17.789120	-0.051526	2.699515
273.713224	2445.323678	17.794125	-0.051577	2.695297
273.434742	2437.344102	17.799130	-0.051520	2.691021
273.155880	2429.428198	17.804135	-0.051463	2.686773
273.232958	2421.457047	17.809139	-0.051472	2.682511
273.137013	2413.466135	17.814144	-0.051449	2.678221
273.124038	2405.505226	17.819149	-0.051441	2.673946
272.856654	2397.536053	17.824154	-0.051386	2.669642
273.183941	2389.493519	17.829159	-0.051442	2.665331
272.910286	2381.586876	17.834163	-0.051386	2.661047
272.825979	2373.594177	17.839168	-0.051365	2.656722
272.976844	2365.604534	17.844173	-0.051387	2.652407
272.827412	2357.640755	17.849178	-0.051354	2.648079
272.409973	2349.743937	17.854183	-0.051271	2.643762
272.518006	2341.753529	17.859187	-0.051286	2.639422
272.423683	2333.778425	17.864192	-0.051264	2.635070
272.359630	2325.807352	17.869197	-0.051246	2.630716
272.627835	2317.773603	17.874202	-0.051291	2.626342
272.662927	2309.799532	17.879207	-0.051292	2.621978
272.541654	2301.874458	17.884211	-0.051265	2.617622
272.132202	2293.941081	17.889216	-0.051183	2.613235
272.346185	2285.934622	17.894221	-0.051218	2.608843
272.095238	2277.969889	17.899226	-0.051166	2.604435
271.995830	2270.025435	17.904231	-0.051142	2.600041
272.286770	2262.037984	17.909235	-0.051191	2.595643
272.145607	2253.979617	17.914240	-0.051159	2.591168
272.218861	2245.978136	17.919245	-0.051168	2.586732
271.812841	2238.082096	17.924250	-0.051087	2.582313
271.974738	2230.099298	17.929255	-0.051112	2.577878
272.221964	2222.093871	17.934259	-0.051153	2.573429
271.919382	2214.180929	17.939264	-0.051091	2.568985
271.993446	2206.195201	17.944269	-0.051100	2.564519
272.106040	2198.249012	17.949274	-0.051115	2.560071
271.800422	2190.335245	17.954279	-0.051053	2.555603
271.627800	2182.380255	17.959283	-0.051016	2.551113
271.504900	2174.403402	17.964288	-0.050988	2.546607
271.437280	2166.448562	17.969293	-0.050970	2.542109
271.028717	2158.523229	17.974298	-0.050889	2.537595
271.298720	2150.484798	17.979303	-0.050934	2.533058
271.029098	2142.548505	17.984307	-0.050878	2.528532
271.032825	2134.561438	17.989312	-0.050874	2.523989
271.072049	2126.626849	17.994317	-0.050876	2.519470
271.048425	2118.662147	17.999322	-0.050866	2.514921
271.046858	2110.652835	18.004327	-0.050861	2.510340
271.479708	2102.614827	18.009331	-0.050936	2.505766
271.097377	2094.732209	18.014336	-0.050860	2.501213
271.255443	2086.736078	18.019341	-0.050884	2.496626
271.099700	2078.801395	18.024346	-0.050850	2.492043
271.570054	2070.751847	18.029351	-0.050932	2.487432
271.373432	2062.865066	18.034355	-0.050890	2.482856
271.217425	2054.908480	18.039360	-0.050856	2.478235
271.292173	2046.944364	18.044365	-0.050864	2.473618
270.726452	2039.084524	18.049370	-0.050754	2.469004
270.699914	2031.076474	18.054375	-0.050744	2.464336
270.645800	2023.140403	18.059379	-0.050729	2.459700
270.437849	2015.174280	18.064384	-0.050685	2.455025
270.291271	2007.233446	18.069389	-0.050652	2.450360
270.152459	1999.244365	18.074394	-0.050621	2.445659
270.031902	1991.316560	18.079399	-0.050593	2.440987
270.291604	1983.309369	18.084403	-0.050636	2.436288
270.003236	1975.340079	18.089408	-0.050577	2.431560
270.291176	1967.311376	18.094413	-0.050626	2.426833
270.312669	1959.345725	18.099418	-0.050625	2.422113
270.044356	1951.439760	18.104423	-0.050569	2.417396
269.737214	1943.541999	18.109427	-0.050507	2.412671
269.619515	1935.546411	18.114432	-0.050480	2.407894
269.593157	1927.599150	18.119437	-0.050470	2.403144
269.560457	1919.637722	18.124442	-0.050458	2.398375
269.431600	1911.693625	18.129447	-0.050429	2.393600
269.734835	1903.674094	18.134451	-0.050480	2.388804
269.396068	1895.739894	18.139456	-0.050412	2.383998
269.433766	1887.800037	18.144461	-0.050414	2.379210
269.626224	1879.805698	18.149466	-0.050445	2.374392
269.568370	1871.845373	18.154471	-0.050429	2.369564
269.735616	1863.883631	18.159475	-0.050454	2.364743
269.706522	1855.939532	18.164480	-0.050444	2.359908
269.421304	1848.058305	18.169485	-0.050386	2.355080
269.293036	1840.103134	18.174490	-0.050356	2.350209
269.218185	1832.110886	18.179495	-0.050337	2.345310
268.973689	1824.219286	18.184499	-0.050287	2.340449
268.852672	1816.243393	18.189504	-0.050259	2.335535
269.092161	1808.240320	18.194509	-0.050298	2.330625
268.567166	1800.376669	18.199514	-0.050195	2.325726
268.665455	1792.385890	18.204519	-0.050208	2.320791
268.791078	1784.422358	18.209523	-0.050226	2.315865
268.411733	1776.517327	18.214528	-0.050151	2.310921
268.739569	1768.482634	18.219533	-0.050206	2.305947
268.502775	1760.575973	18.224538	-0.050157	2.300993
268.280120	1752.664085	18.229543	-0.050110	2.296026
268.178836	1744.716575	18.234547	-0.050086	2.291037
268.158272	1736.701010	18.239552	-0.050077	2.286001
268.248803	1728.770925	18.244557	-0.050089	2.281018
268.402329	1720.807069	18.249562	-0.050112	2.276007
268.269900	1712.835566	18.254567	-0.050082	2.270956
268.229611	1704.871740	18.259571	-0.050070	2.265907
268.211109	1696.910608	18.264576	-0.050061	2.260850
268.266313	1688.983935	18.269581	-0.050066	2.255810
267.965416	1681.076121	18.274586	-0.050005	2.250738
268.035087	1673.080489	18.279591	-0.050013	2.245633
268.371969	1665.118277	18.284595	-0.050070	2.240561
267.884709	1657.252035	18.289600	-0.049974	2.235465
267.986759	1649.286970	18.294605	-0.049988	2.230347
267.779831	1641.358025	18.299610	-0.049944	2.225213
267.550895	1633.436633	18.304615	-0.049896	2.220069
267.321352	1625.531906	18.309619	-0.049848	2.214925
267.372328	1617.533285	18.314624	-0.049853	2.209733
267.442250	1609.563175	18.319629	-0.049860	2.204549
267.494898	1601.618495	18.324634	-0.049865	2.199368
267.481269	1593.679737	18.329639	-0.049857	2.194172
267.558836	1585.733489	18.334643	-0.049866	2.188968
267.175155	1577.809876	18.339648	-0.049790	2.183722
266.998041	1569.918444	18.344653	-0.049752	2.178505
267.096220	1561.943922	18.349658	-0.049765	2.173247
267.243578	1553.960859	18.354663	-0.049787	2.167974
267.106135	1546.044928	18.359667	-0.049756	2.162706
266.955398	1538.124498	18.364672	-0.049723	2.157421
266.997928	1530.196282	18.369677	-0.049726	2.152137
266.671163	1522.298861	18.374682	-0.049660	2.146824
266.721850	1514.315463	18.379687	-0.049664	2.141477
266.986154	1506.333210	18.384691	-0.049708	2.136138
266.798441	1498.408190	18.389696	-0.049668	2.130781
266.627140	1490.510083	18.394701	-0.049630	2.125429
266.622431	1482.582533	18.399706	-0.049624	2.120061
266.302602	1474.694544	18.404711	-0.049560	2.114674
266.294883	1466.721557	18.409715	-0.049553	2.109247
266.191268	1458.758797	18.414720	-0.049528	2.103803
266.612629	1450.747368	18.419725	-0.049602	2.098364
266.712696	1442.795006	18.424730	-0.049615	2.092919
266.502253	1434.904692	18.429735	-0.049571	2.087472
266.289327	1427.035024	18.434739	-0.049526	2.082025
266.651409	1419.013799	18.439744	-0.049588	2.076516
266.495864	1411.149657	18.444749	-0.049554	2.071049
266.518923	1403.193146	18.449754	-0.049553	2.065522
266.094268	1395.359216	18.454759	-0.049469	2.060019
266.084409	1387.421268	18.459763	-0.049462	2.054472
265.893529	1379.488011	18.464768	-0.049421	2.048894
266.060276	1371.526637	18.469773	-0.049447	2.043318
266.369719	1363.552274	18.474778	-0.049499	2.037733
266.079151	1355.672315	18.479783	-0.049440	2.032136
265.927665	1347.778936	18.484787	-0.049406	2.026529
265.903909	1339.836995	18.489792	-0.049397	2.020885
266.108105	1331.879683	18.494797	-0.049430	2.015239
266.008796	1323.951829	18.499802	-0.049406	2.009565
266.138690	1316.017971	18.504807	-0.049425	2.003896
265.943462	1308.159427	18.509811	-0.049383	1.998230
266.337419	1300.148000	18.514816	-0.049451	1.992500
266.078530	1292.304024	18.519821	-0.049398	1.986805
266.092737	1284.376695	18.524826	-0.049396	1.981063
265.780724	1276.516008	18.529831	-0.049332	1.975317
266.086439	1268.528699	18.534835	-0.049384	1.969529
265.437091	1260.722036	18.539840	-0.049258	1.963752
265.283834	1252.833028	18.544845	-0.049224	1.957952
264.994413	1244.939868	18.549850	-0.049165	1.952116
265.129757	1236.961071	18.554855	-0.049185	1.946246
264.927073	1229.062048	18.559859	-0.049142	1.940381
264.391574	1221.205189	18.564864	-0.049037	1.934491
264.704236	1213.216731	18.569869	-0.049090	1.928581
264.523668	1205.309005	18.574874	-0.049051	1.922657
264.701971	1197.354278	18.579879	-0.049079	1.916720
264.508146	1189.491514	18.584883	-0.049038	1.910792
264.573363	1181.518545	18.589888	-0.049045	1.904791
264.343258	1173.676801	18.594893	-0.048997	1.898838
264.202367	1165.758041	18.599898	-0.048966	1.892817
264.169984	1157.840629	18.604903	-0.048954	1.886790
263.935605	1149.977530	18.609907	-0.048906	1.880762
263.729592	1142.071549	18.614912	-0.048862	1.874685
264.287453	1134.065608	18.619917	-0.048961	1.868601
263.926616	1126.209531	18.624922	-0.048888	1.862505
263.722292	1118.322565	18.629927	-0.048845	1.856383
263.702242	1110.414338	18.634931	-0.048836	1.850246
263.626955	1102.516800	18.639936	-0.048817	1.844091
263.738183	1094.616709	18.644941	-0.048833	1.837935
263.750240	1086.704746	18.649946	-0.048830	1.831737
263.716707	1078.793845	18.654951	-0.048818	1.825514
263.845906	1070.894017	18.659955	-0.048837	1.819298
263.436819	1063.073500	18.664960	-0.048756	1.813057
263.911389	1055.069427	18.669965	-0.048839	1.806758
263.786476	1047.218522	18.674970	-0.048810	1.800485
263.315558	1039.413775	18.679975	-0.048718	1.794184
263.377585	1031.476422	18.684979	-0.048724	1.787820
263.206549	1023.592135	18.689984	-0.048687	1.781447
263.096173	1015.719768	18.694989	-0.048661	1.775069
262.965002	1007.830800	18.699994	-0.048632	1.768651
262.864048	999.953568	18.704999	-0.048608	1.762224
262.861764	992.081851	18.710003	-0.048602	1.755790
262.563812	984.230980	18.715008	-0.048541	1.749311
262.692613	976.317449	18.720013	-0.048560	1.742812
262.912966	968.384936	18.725018	-0.048596	1.736285
262.707960	960.528080	18.730023	-0.048553	1.729740
262.894705	952.616552	18.735027	-0.048582	1.723176
262.639352	944.810266	18.740032	-0.048530	1.716617
262.439273	936.975520	18.745037	-0.048487	1.710016
262.056536	929.149007	18.750042	-0.048411	1.703372
262.141582	921.236550	18.755047	-0.048421	1.696692
262.259869	913.325803	18.760051	-0.048438	1.689992
261.987808	905.480240	18.765056	-0.048382	1.683267
262.198924	897.589284	18.770061	-0.048417	1.676542
262.152224	889.720507	18.775066	-0.048403	1.669775
262.432052	881.786469	18.780071	-0.048450	1.662968
262.014124	874.036652	18.785075	-0.048367	1.656196
261.823825	866.184418	18.790080	-0.048326	1.649339
261.981970	858.293043	18.795085	-0.048350	1.642468
261.658954	850.507200	18.800090	-0.048285	1.635593
261.502215	842.632588	18.805095	-0.048251	1.628634
261.619789	834.745787	18.810099	-0.048267	1.621673
261.157733	826.953837	18.815104	-0.048176	1.614684
261.410002	819.042087	18.820109	-0.048218	1.607660
261.455159	811.171494	18.825114	-0.048221	1.600613
261.255377	803.371460	18.830119	-0.048179	1.593562
261.050252	795.555968	18.835123	-0.048136	1.586465
260.790569	787.751831	18.840128	-0.048082	1.579338
260.814167	779.903000	18.845133	-0.048081	1.572180
260.754334	772.044019	18.850138	-0.048065	1.564967
260.784663	764.210863	18.855143	-0.048066	1.557758
260.738677	756.377586	18.860147	-0.048052	1.550505
260.549286	748.550118	18.865152	-0.048011	1.543200
260.592462	740.714333	18.870157	-0.048014	1.535889
260.825127	732.819472	18.875162	-0.048052	1.528516
261.274076	724.912538	18.880167	-0.048131	1.521129
260.868863	717.212591	18.885171	-0.048050	1.513771
260.615999	709.421224	18.890176	-0.047998	1.506313
260.422636	701.658422	18.895181	-0.047957	1.498854
260.127744	693.883833	18.900186	-0.047897	1.491331
260.564883	685.960204	18.905191	-0.047973	1.483742
259.800221	678.314848	18.910195	-0.047826	1.476192
259.693836	670.470000	18.915200	-0.047801	1.468514
259.853069	662.611863	18.920205	-0.047825	1.460825
260.131207	654.756581	18.925210	-0.047872	1.453118
260.034615	646.965570	18.930215	-0.047849	1.445373
259.724338	639.252555	18.935219	-0.047786	1.437628
259.859292	631.415254	18.940224	-0.047806	1.429791
259.640112	623.670914	18.945229	-0.047760	1.421945
259.482314	615.911720	18.950234	-0.047726	1.414050
259.411992	608.122654	18.955239	-0.047707	1.406096
259.213415	600.397415	18.960243	-0.047665	1.398139
259.457910	592.550704	18.965248	-0.047706	1.390088
259.185040	584.824161	18.970253	-0.047650	1.382026
258.956433	577.100959	18.975258	-0.047602	1.373927
258.780899	569.334102	18.980263	-0.047564	1.365743
258.819323	561.583466	18.985267	-0.047567	1.357565
258.510113	553.865101	18.990272	-0.047504	1.349310
258.782519	546.053145	18.995277	-0.047549	1.341008
258.852099	538.293216	19.000282	-0.047557	1.332674
258.960940	530.521221	19.005287	-0.047572	1.324282
259.004324	522.805386	19.010291	-0.047576	1.315885
258.758192	515.021909	19.015296	-0.047525	1.307307
258.627388	507.319787	19.020301	-0.047495	1.298783
258.782883	499.556694	19.025306	-0.047519	1.290189
258.515152	491.896286	19.030311	-0.047464	1.281572
258.693784	484.161935	19.035315	-0.047492	1.272899
258.516150	476.471121	19.040320	-0.047454	1.264147
258.432850	468.804875	19.045325	-0.047434	1.255380
258.077668	461.166937	19.050330	-0.047362	1.246531
257.837050	453.522109	19.055335	-0.047313	1.237633
257.935677	445.809001	19.060339	-0.047326	1.228659
257.626825	438.160581	19.065344	-0.047263	1.219612
257.672462	430.474761	19.070349	-0.047267	1.210526
257.850106	422.768240	19.075354	-0.047295	1.201372
257.863890	415.111184	19.080359	-0.047292	1.192175
257.804076	407.471273	19.085363	-0.047276	1.182912
257.699153	399.837245	19.090368	-0.047252	1.173573
258.127412	392.123013	19.095373	-0.047326	1.164172
257.785054	384.571377	19.100378	-0.047258	1.154734
257.448622	376.980671	19.105383	-0.047190	1.145170
257.187518	369.417912	19.110387	-0.047136	1.135577
257.048701	361.804435	19.115392	-0.047106	1.125864
256.996934	354.223233	19.120397	-0.047091	1.116127
256.844951	346.643940	19.125402	-0.047058	1.106285
256.714071	339.083330	19.130407	-0.047028	1.096383
256.627364	331.521711	19.135411	-0.047007	1.086400
256.406807	323.991278	19.140416	-0.046961	1.076335
256.568755	316.398041	19.145421	-0.046986	1.066180
256.838231	308.801861	19.150426	-0.047032	1.055948
256.461510	301.337436	19.155431	-0.046957	1.045643
256.645334	293.804063	19.160435	-0.046986	1.035275
256.332991	286.344394	19.165440	-0.046923	1.024785
255.985127	278.921198	19.170445	-0.046853	1.014229
255.812819	271.452854	19.175450	-0.046816	1.003540
255.745532	263.979232	19.180455	-0.046799	0.992756
255.918954	256.461192	19.185459	-0.046826	0.981849
255.507627	249.085956	19.190464	-0.046745	0.970880
255.502163	241.651356	19.195469	-0.046739	0.959803
255.422060	234.254082	19.200474	-0.046719	0.948634
255.433026	226.840806	19.205479	-0.046716	0.937331
255.308457	219.490476	19.210483	-0.046688	0.925951
255.279990	212.138392	19.215488	-0.046678	0.914453
255.235719	204.788319	19.220493	-0.046665	0.902808
255.060619	197.496138	19.225498	-0.046627	0.891066
255.085509	190.184190	19.230503	-0.046627	0.879193
255.030888	182.916826	19.235507	-0.046612	0.867208
254.885116	175.673644	19.240512	-0.046580	0.855069
254.816696	168.449028	19.245517	-0.046563	0.842809
254.628618	161.264591	19.250522	-0.046523	0.830402
254.349719	154.107855	19.255527	-0.046467	0.817827
254.405425	146.928660	19.260531	-0.046472	0.805121
254.095559	139.846604	19.265536	-0.046410	0.792269
254.041224	132.751948	19.270541	-0.046395	0.779266
253.831781	125.706123	19.275546	-0.046351	0.766083
253.928194	118.640666	19.280551	-0.046365	0.752734
253.690177	111.667495	19.285555	-0.046316	0.739209
253.422785	104.733245	19.290560	-0.046262	0.725498
253.612178	97.764539	19.295565	-0.046292	0.711617
253.367875	90.910534	19.300570	-0.046242	0.697538
253.175204	84.080470	19.305575	-0.046202	0.683238
252.973635	77.479519	19.310579	-0.046160	0.669121