Mon Apr 19 09:18:00 2021

Number of Points = 3639
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.565950	-0.115304	0.000000	-0.000060	0.309273

2.439395	-0.092222	0.005005	-0.000036	0.309273
2.658519	-0.132091	0.010010	-0.000077	0.309273
2.829409	-0.165661	0.015014	-0.000109	0.309261
2.976930	-0.193630	0.020019	-0.000136	0.309255
2.524187	-0.107079	0.025024	-0.000052	0.309275
2.425799	-0.088759	0.030029	-0.000034	0.309277
2.544766	-0.109931	0.035034	-0.000056	0.309279
2.389823	-0.089778	0.040038	-0.000027	0.309241
2.728036	-0.219029	0.045043	-0.000090	0.308924
3.125983	-0.292618	0.050048	-0.000164	0.308917
3.082738	-0.286155	0.055053	-0.000156	0.308911
3.056836	-0.279514	0.060058	-0.000151	0.308919
2.974672	-0.266963	0.065062	-0.000135	0.308908
2.528373	-0.178341	0.070067	-0.000052	0.308943
2.228116	-0.123127	0.075072	0.000004	0.308946
2.333808	-0.198645	0.080077	-0.000016	0.308682
2.559256	-0.251119	0.085082	-0.000058	0.308628
2.256626	-0.197269	0.090086	-0.000002	0.308622
2.263560	-0.196975	0.095091	-0.000003	0.308630
2.387591	-0.220337	0.100096	-0.000026	0.308626
2.608629	-0.262681	0.105101	-0.000067	0.308615
2.798405	-0.351279	0.110106	-0.000102	0.308361
2.519679	-0.313850	0.115110	-0.000050	0.308299
1.940727	-0.203280	0.120115	0.000058	0.308324
1.984322	-0.211532	0.125120	0.000049	0.308322
2.084819	-0.232526	0.130125	0.000031	0.308309
2.122933	-0.287797	0.135130	0.000024	0.308082
2.017845	-0.280791	0.140134	0.000043	0.308025
1.799031	-0.238232	0.145139	0.000084	0.308038
2.244891	-0.322174	0.150144	0.000001	0.308024
2.158985	-0.336981	0.155149	0.000017	0.307881
1.935816	-0.335947	0.160154	0.000059	0.307695
1.562598	-0.268017	0.165158	0.000128	0.307696
1.951058	-0.338825	0.170163	0.000056	0.307694
1.737686	-0.324388	0.175168	0.000096	0.307580
1.501287	-0.321620	0.180173	0.000140	0.307390
1.921241	-0.399050	0.185178	0.000062	0.307385
2.499453	-0.510401	0.190182	-0.000046	0.307355
2.656680	-0.599868	0.195187	-0.000075	0.307068
2.257455	-0.532392	0.200192	-0.000001	0.307044
1.895622	-0.466819	0.205197	0.000067	0.307043
2.501021	-0.630433	0.210202	-0.000046	0.306790
2.198953	-0.583633	0.215206	0.000010	0.306752
2.128759	-0.574062	0.220211	0.000024	0.306737
1.950464	-0.605847	0.225216	0.000057	0.306434
1.982901	-0.614578	0.230221	0.000051	0.306420
1.517796	-0.540185	0.235226	0.000137	0.306372
1.462329	-0.578663	0.240230	0.000148	0.306142
1.461509	-0.576783	0.245235	0.000148	0.306150
1.632870	-0.636280	0.250240	0.000116	0.306016
1.978709	-0.743869	0.255245	0.000052	0.305804
1.304381	-0.614322	0.260250	0.000177	0.305837
1.336268	-0.662509	0.265254	0.000172	0.305637
1.345657	-0.675106	0.270259	0.000170	0.305585
1.190222	-0.658662	0.275264	0.000199	0.305529
1.296887	-0.742625	0.280269	0.000179	0.305223
1.648089	-0.804995	0.285274	0.000114	0.305229
1.352293	-0.802357	0.290278	0.000169	0.304987
1.626905	-0.870449	0.295283	0.000118	0.304900
1.312168	-0.840006	0.300288	0.000176	0.304773
1.734912	-0.960338	0.305293	0.000098	0.304566
1.581534	-0.944150	0.310298	0.000126	0.304511
1.683248	-1.009520	0.315302	0.000108	0.304287
1.773763	-1.039957	0.320307	0.000091	0.304221
1.976077	-1.134947	0.325312	0.000053	0.303944
1.911843	-1.142175	0.330317	0.000065	0.303853
1.829166	-1.173917	0.335322	0.000081	0.303630
1.352973	-1.105470	0.340326	0.000169	0.303544
1.688533	-1.215820	0.345331	0.000107	0.303308
1.190989	-1.141793	0.350336	0.000200	0.303230
1.576436	-1.255534	0.355341	0.000128	0.303021
1.619150	-1.298466	0.360346	0.000120	0.302853
1.291201	-1.273024	0.365350	0.000181	0.302690
1.376633	-1.331088	0.370355	0.000165	0.302486
1.727327	-1.418507	0.375360	0.000100	0.302373
1.524548	-1.444052	0.380365	0.000138	0.302074
1.731641	-1.499284	0.385370	0.000099	0.301989
1.503375	-1.505228	0.390374	0.000142	0.301762
1.248555	-1.493764	0.395379	0.000189	0.301594
1.531571	-1.580720	0.400384	0.000137	0.301424
1.374370	-1.606098	0.405389	0.000166	0.301165
1.878477	-1.725964	0.410394	0.000072	0.301029
1.544262	-1.714243	0.415398	0.000135	0.300793
1.643255	-1.767897	0.420403	0.000116	0.300621
2.173011	-1.895374	0.425408	0.000018	0.300471
1.976246	-1.917383	0.430413	0.000055	0.300192
1.907034	-1.950804	0.435418	0.000067	0.299970
1.843633	-1.978855	0.440422	0.000079	0.299779
1.906502	-2.035474	0.445427	0.000068	0.299561
1.759694	-2.060351	0.450432	0.000095	0.299311
1.748083	-2.100575	0.455437	0.000097	0.299106
1.886974	-2.166473	0.460442	0.000072	0.298909
2.243563	-2.293318	0.465446	0.000005	0.298609
1.746039	-2.251168	0.470451	0.000098	0.298375
1.447948	-2.232969	0.475456	0.000153	0.298200
1.202104	-2.226028	0.480461	0.000199	0.298017
1.505201	-2.346840	0.485466	0.000143	0.297697
1.546627	-2.403238	0.490470	0.000135	0.297459
1.290671	-2.398723	0.495475	0.000183	0.297255
0.982262	-2.383410	0.500480	0.000240	0.297056
1.402292	-2.519969	0.505485	0.000162	0.296763
1.869521	-2.657424	0.510490	0.000076	0.296506
1.250236	-2.591623	0.515494	0.000191	0.296278
1.342641	-2.654730	0.520499	0.000174	0.296051
1.210047	-2.678216	0.525504	0.000198	0.295818
1.458741	-2.775984	0.530509	0.000152	0.295561
0.951050	-2.731253	0.535514	0.000247	0.295328
1.259125	-2.840909	0.540518	0.000190	0.295065
0.942374	-2.831944	0.545523	0.000249	0.294826
0.593861	-2.816426	0.550528	0.000313	0.294591
0.639557	-2.884180	0.555533	0.000305	0.294299
0.846600	-2.973525	0.560538	0.000267	0.294044
0.760400	-3.011133	0.565542	0.000283	0.293782
1.086047	-3.122441	0.570547	0.000222	0.293525
1.283254	-3.212546	0.575552	0.000186	0.293257
0.683207	-3.150998	0.580557	0.000297	0.293022
0.648642	-3.204790	0.585562	0.000304	0.292725
0.838693	-3.300990	0.590566	0.000269	0.292420
1.241207	-3.431436	0.595571	0.000194	0.292136
1.319919	-3.500836	0.600576	0.000179	0.291863
0.789389	-3.461683	0.605581	0.000278	0.291579
-2.045263	-3.003808	0.610586	0.000805	0.291294
-5.226010	-2.459571	0.615590	0.001397	0.291125
-4.680762	-2.600639	0.620595	0.001296	0.290916
-5.086304	-2.547377	0.625600	0.001372	0.290814
-5.186998	-2.575499	0.630605	0.001390	0.290583
-5.407013	-2.539873	0.635610	0.001431	0.290561
-5.753909	-2.546826	0.640614	0.001496	0.290212
-5.532363	-2.599378	0.645619	0.001455	0.290150
-5.737943	-2.616394	0.650624	0.001493	0.289879
-6.143731	-2.561894	0.655629	0.001569	0.289782
-6.997701	-2.447357	0.660634	0.001728	0.289579
-6.830331	-2.495046	0.665638	0.001697	0.289492
-7.490927	-2.413607	0.670643	0.001820	0.289299
-7.719762	-2.380370	0.675648	0.001862	0.289257
-8.081690	-2.377625	0.680653	0.001930	0.288941
-7.373720	-2.506965	0.685658	0.001798	0.288938
-7.879838	-2.475972	0.690662	0.001892	0.288632
-8.507656	-2.360035	0.695667	0.002009	0.288641
-7.834431	-2.534259	0.700672	0.001884	0.288380
-8.716675	-2.386310	0.705677	0.002048	0.288318
-8.981203	-2.370698	0.710682	0.002097	0.288154
-8.779662	-2.435753	0.715686	0.002060	0.288011
-8.442843	-2.528018	0.720691	0.001997	0.287855
-9.414672	-2.385518	0.725696	0.002178	0.287683
-9.646375	-2.352618	0.730701	0.002221	0.287637
-9.308309	-2.468065	0.735706	0.002159	0.287365
-9.537920	-2.428636	0.740710	0.002201	0.287353
-9.488125	-2.495965	0.745715	0.002192	0.287059
-10.101537	-2.386592	0.750720	0.002306	0.287048
-10.745729	-2.300356	0.755725	0.002426	0.286892
-10.704465	-2.333005	0.760730	0.002419	0.286765
-11.341854	-2.214668	0.765734	0.002537	0.286777
-10.608983	-2.416788	0.770739	0.002401	0.286429
-10.728011	-2.397940	0.775744	0.002423	0.286415
-11.338583	-2.323226	0.780749	0.002537	0.286231
-11.503761	-2.313197	0.785754	0.002568	0.286130
-12.004519	-2.221100	0.790758	0.002661	0.286135
-11.973614	-2.288086	0.795763	0.002655	0.285824
-11.690796	-2.342728	0.800768	0.002603	0.285808
-12.020954	-2.303811	0.805773	0.002664	0.285701
-12.495733	-2.242512	0.810778	0.002752	0.285574
-12.615922	-2.223113	0.815782	0.002775	0.285561
-12.592674	-2.273152	0.820787	0.002771	0.285329
-12.555992	-2.302861	0.825792	0.002764	0.285211
-12.778103	-2.267289	0.830797	0.002805	0.285187
-12.487482	-2.377045	0.835802	0.002751	0.284898
-12.745209	-2.334151	0.840806	0.002799	0.284877
-12.906309	-2.341990	0.845811	0.002829	0.284688
-12.940452	-2.363002	0.850816	0.002836	0.284550
-12.844788	-2.389650	0.855821	0.002818	0.284502
-13.112857	-2.387984	0.860826	0.002868	0.284263
-13.579665	-2.302468	0.865830	0.002955	0.284266
-13.568679	-2.344642	0.870835	0.002953	0.284061
-14.111327	-2.265887	0.875840	0.003054	0.283959
-14.140950	-2.262694	0.880845	0.003059	0.283948
-14.126282	-2.322053	0.885850	0.003057	0.283659
-14.133004	-2.327521	0.890854	0.003058	0.283624
-13.979538	-2.382911	0.895859	0.003030	0.283484
-14.202238	-2.377304	0.900864	0.003071	0.283305
-14.515606	-2.320779	0.905869	0.003129	0.283303
-14.862004	-2.305138	0.910874	0.003194	0.283061
-15.147597	-2.261014	0.915878	0.003247	0.283021
-14.771085	-2.344496	0.920883	0.003177	0.282944
-15.303533	-2.296480	0.925888	0.003276	0.282694
-15.596432	-2.247622	0.930893	0.003331	0.282671
-15.026973	-2.384412	0.935898	0.003225	0.282500
-15.285869	-2.366647	0.940902	0.003273	0.282350
-15.830463	-2.265309	0.945907	0.003375	0.282362
-15.885248	-2.316976	0.950912	0.003385	0.282045
-15.692168	-2.358027	0.955917	0.003349	0.282015
-15.751819	-2.366432	0.960922	0.003360	0.281916
-16.622413	-2.240449	0.965926	0.003522	0.281749
-16.800627	-2.205439	0.970931	0.003555	0.281763
-16.468410	-2.305732	0.975936	0.003494	0.281557
-17.155391	-2.210167	0.980941	0.003621	0.281406
-16.913662	-2.248807	0.985946	0.003577	0.281434
-17.364632	-2.216222	0.990950	0.003660	0.281179
-17.962687	-2.115574	0.995955	0.003772	0.281137
-17.529824	-2.194991	1.000960	0.003691	0.281133
-17.091086	-2.333893	1.005965	0.003610	0.280829
-17.434350	-2.276443	1.010970	0.003674	0.280803
-17.760451	-2.226927	1.015974	0.003734	0.280752
-17.848477	-2.246044	1.020979	0.003751	0.280571
-18.033306	-2.209229	1.025984	0.003785	0.280587
-18.458086	-2.155177	1.030989	0.003864	0.280467
-18.782421	-2.137009	1.035994	0.003925	0.280256
-18.524004	-2.187011	1.040998	0.003877	0.280241
-18.882234	-2.142274	1.046003	0.003943	0.280135
-18.841226	-2.191737	1.051008	0.003936	0.279918
-18.749199	-2.208469	1.056013	0.003919	0.279917
-18.665936	-2.255146	1.061018	0.003903	0.279754
-19.451645	-2.144742	1.066022	0.004050	0.279586
-19.239533	-2.181855	1.071027	0.004010	0.279593
-19.286984	-2.206798	1.076032	0.004019	0.279419
-20.163321	-2.069702	1.081037	0.004182	0.279304
-19.649990	-2.162086	1.086042	0.004087	0.279308
-19.536177	-2.226273	1.091046	0.004066	0.279083
-20.293302	-2.108829	1.096051	0.004207	0.278978
-20.206916	-2.125168	1.101056	0.004191	0.278974
-20.182087	-2.174196	1.106061	0.004186	0.278743
-20.467753	-2.135496	1.111066	0.004239	0.278674
-20.180741	-2.192879	1.116070	0.004186	0.278647
-20.085287	-2.264363	1.121075	0.004168	0.278365
-20.262667	-2.239337	1.126080	0.004201	0.278327
-20.733056	-2.165353	1.131085	0.004289	0.278267
-20.852387	-2.185228	1.136090	0.004311	0.278050
-20.870383	-2.186264	1.141094	0.004314	0.278028
-20.740920	-2.236438	1.146099	0.004290	0.277889
-20.818720	-2.261678	1.151104	0.004305	0.277683
-20.863254	-2.253739	1.156109	0.004313	0.277682
-20.680525	-2.331416	1.161114	0.004279	0.277450
-21.245397	-2.246639	1.166118	0.004385	0.277356
-21.135059	-2.280110	1.171123	0.004364	0.277286
-21.405870	-2.275006	1.176128	0.004414	0.277056
-21.614267	-2.239225	1.181133	0.004453	0.277044
-21.763078	-2.242106	1.186138	0.004481	0.276888
-22.329899	-2.160130	1.191142	0.004587	0.276777
-21.901641	-2.239211	1.196147	0.004507	0.276771
-21.970071	-2.280721	1.201152	0.004520	0.276488
-22.761529	-2.146486	1.206157	0.004667	0.276437
-22.518169	-2.194733	1.211162	0.004622	0.276416
-22.980660	-2.163545	1.216166	0.004708	0.276138
-22.689649	-2.220092	1.221171	0.004654	0.276119
-22.398644	-2.293705	1.226176	0.004600	0.276010
-23.026929	-2.218310	1.231181	0.004717	0.275806
-23.122518	-2.198765	1.236186	0.004735	0.275818
-23.649333	-2.131785	1.241190	0.004833	0.275666
-23.083501	-2.253987	1.246195	0.004727	0.275564
-23.192854	-2.233464	1.251200	0.004748	0.275568
-23.206106	-2.300664	1.256205	0.004750	0.275201
-23.273370	-2.286186	1.261210	0.004763	0.275213
-23.819279	-2.213219	1.266214	0.004865	0.275074
-23.957690	-2.221420	1.271219	0.004890	0.274898
-23.463371	-2.312150	1.276224	0.004798	0.274894
-23.800270	-2.306537	1.281229	0.004861	0.274600
-23.945034	-2.286848	1.286234	0.004888	0.274565
-24.115218	-2.272465	1.291238	0.004920	0.274478
-24.385984	-2.259677	1.296243	0.004970	0.274285
-24.347774	-2.267470	1.301248	0.004963	0.274280
-25.062991	-2.184961	1.306253	0.005096	0.274029
-24.951131	-2.216867	1.311258	0.005076	0.273968
-25.428518	-2.129040	1.316262	0.005165	0.273973
-25.692131	-2.139094	1.321267	0.005214	0.273666
-25.517067	-2.173386	1.326272	0.005181	0.273653
-25.452249	-2.195339	1.331277	0.005169	0.273599
-25.678900	-2.204182	1.336282	0.005211	0.273334
-25.808316	-2.181340	1.341286	0.005235	0.273330
-25.833450	-2.199527	1.346291	0.005240	0.273209
-26.044822	-2.193259	1.351296	0.005280	0.273038
-26.176981	-2.170841	1.356301	0.005304	0.273029
-26.084698	-2.227137	1.361306	0.005287	0.272820
-25.867841	-2.292937	1.366310	0.005247	0.272679
-26.108837	-2.256789	1.371315	0.005292	0.272638
-26.558344	-2.220909	1.376320	0.005375	0.272395
-26.712319	-2.192786	1.381325	0.005404	0.272395
-26.972331	-2.172684	1.386330	0.005453	0.272250
-27.046492	-2.195596	1.391334	0.005466	0.272056
-27.079816	-2.188382	1.396339	0.005473	0.272062
-27.006961	-2.240528	1.401344	0.005459	0.271855
-27.746326	-2.120486	1.406349	0.005597	0.271778
-27.520438	-2.160086	1.411354	0.005555	0.271786
-28.061887	-2.122738	1.416358	0.005656	0.271460
-28.400846	-2.059793	1.421363	0.005719	0.271466
-27.878216	-2.161229	1.426368	0.005622	0.271432
-27.829187	-2.226792	1.431373	0.005613	0.271129
-28.118119	-2.171723	1.436378	0.005666	0.271143
-28.792880	-2.064611	1.441382	0.005792	0.271059
-28.378301	-2.183690	1.446387	0.005715	0.270826
-28.121763	-2.232093	1.451392	0.005667	0.270816
-29.378939	-2.029596	1.456397	0.005901	0.270676
-28.761605	-2.159814	1.461402	0.005786	0.270580
-28.451751	-2.220032	1.466406	0.005729	0.270559
-29.017995	-2.173777	1.471411	0.005834	0.270255
-28.834852	-2.214375	1.476416	0.005800	0.270216
-28.888661	-2.221028	1.481421	0.005810	0.270127
-29.004172	-2.243168	1.486426	0.005832	0.269896
-29.546305	-2.143297	1.491430	0.005933	0.269902
-29.442996	-2.202186	1.496435	0.005914	0.269687
-29.659431	-2.182705	1.501440	0.005954	0.269580
-29.780509	-2.163714	1.506445	0.005976	0.269563
-29.896919	-2.189149	1.511450	0.005998	0.269313
-30.283350	-2.120462	1.516454	0.006070	0.269304
-30.578771	-2.081093	1.521459	0.006125	0.269227
-30.526884	-2.137843	1.526464	0.006116	0.268972
-30.481372	-2.147449	1.531469	0.006107	0.268964
-30.725840	-2.127756	1.536474	0.006153	0.268831
-31.305578	-2.052870	1.541478	0.006261	0.268666
-31.094403	-2.091566	1.546483	0.006221	0.268664
-30.894355	-2.162457	1.551488	0.006184	0.268478
-31.865331	-2.011080	1.556493	0.006365	0.268342
-31.113741	-2.147827	1.561498	0.006225	0.268341
-31.088637	-2.196772	1.566502	0.006220	0.268101
-31.467442	-2.138071	1.571507	0.006291	0.268046
-31.632802	-2.115301	1.576512	0.006322	0.268006
-31.955000	-2.112633	1.581517	0.006382	0.267704
-31.406581	-2.212926	1.586522	0.006280	0.267701
-32.154355	-2.102502	1.591526	0.006419	0.267562
-32.285006	-2.110413	1.596531	0.006443	0.267390
-31.918954	-2.178742	1.601536	0.006375	0.267381
-32.490342	-2.122410	1.606541	0.006482	0.267122
-32.302766	-2.166564	1.611546	0.006447	0.267068
-32.371922	-2.159624	1.616550	0.006460	0.267037
-32.926081	-2.104426	1.621555	0.006563	0.266789
-33.129896	-2.063996	1.626560	0.006601	0.266807
-33.105517	-2.090946	1.631565	0.006596	0.266685
-33.161785	-2.122907	1.636570	0.006607	0.266456
-33.345875	-2.091293	1.641574	0.006641	0.266445
-33.329020	-2.128233	1.646579	0.006638	0.266261
-33.299160	-2.154885	1.651584	0.006633	0.266145
-33.589613	-2.103309	1.656589	0.006687	0.266138
-33.801602	-2.116964	1.661594	0.006726	0.265854
-34.025203	-2.080505	1.666598	0.006768	0.265831
-33.913965	-2.112869	1.671603	0.006747	0.265764
-34.219386	-2.092332	1.676608	0.006804	0.265573
-34.085572	-2.118862	1.681613	0.006779	0.265561
-34.142719	-2.139031	1.686618	0.006790	0.265394
-34.430666	-2.120404	1.691622	0.006844	0.265210
-33.863452	-2.227607	1.696627	0.006738	0.265187
-33.898822	-2.275971	1.701632	0.006745	0.264888
-34.739591	-2.121539	1.706637	0.006901	0.264896
-34.915694	-2.115080	1.711642	0.006934	0.264756
-35.078108	-2.118053	1.716646	0.006964	0.264578
-35.161057	-2.101892	1.721651	0.006980	0.264583
-35.123757	-2.150911	1.726656	0.006973	0.264352
-35.530586	-2.089095	1.731661	0.007049	0.264285
-34.951303	-2.209060	1.736666	0.006941	0.264205
-36.124861	-2.039981	1.741670	0.007160	0.263961
-36.216353	-2.023046	1.746675	0.007177	0.263962
-35.705324	-2.138929	1.751680	0.007082	0.263836
-36.361685	-2.052863	1.756685	0.007204	0.263653
-36.176210	-2.086229	1.761690	0.007169	0.263655
-35.986322	-2.165965	1.766694	0.007134	0.263406
-36.505035	-2.088105	1.771699	0.007231	0.263315
-36.349754	-2.123095	1.776704	0.007202	0.263278
-36.628143	-2.118193	1.781709	0.007254	0.263026
-36.588615	-2.122498	1.786714	0.007246	0.263042
-36.775911	-2.121968	1.791718	0.007281	0.262857
-37.316937	-2.053761	1.796723	0.007382	0.262690
-36.599091	-2.184624	1.801728	0.007248	0.262688
-37.106970	-2.146339	1.806733	0.007343	0.262390
-37.454530	-2.085079	1.811738	0.007408	0.262379
-37.105152	-2.168583	1.816742	0.007343	0.262268
-37.214571	-2.191028	1.821747	0.007363	0.262034
-37.416984	-2.152794	1.826752	0.007401	0.262042
-37.764428	-2.133827	1.831757	0.007466	0.261797
-37.747927	-2.142564	1.836762	0.007463	0.261765
-37.602241	-2.188918	1.841766	0.007436	0.261655
-37.724488	-2.213758	1.846771	0.007458	0.261394
-37.505131	-2.249270	1.851776	0.007418	0.261418
-37.707828	-2.268263	1.856781	0.007455	0.261108
-38.014699	-2.213437	1.861786	0.007512	0.261102
-38.759831	-2.101732	1.866790	0.007651	0.260970
-39.148273	-2.059415	1.871795	0.007724	0.260812
-38.726796	-2.137955	1.876800	0.007645	0.260802
-38.732510	-2.180466	1.881805	0.007646	0.260560
-38.471033	-2.228820	1.886810	0.007598	0.260555
-38.555056	-2.246482	1.891814	0.007613	0.260372
-39.494676	-2.105648	1.896819	0.007788	0.260204
-38.871781	-2.222972	1.901824	0.007672	0.260181
-39.054046	-2.244830	1.906829	0.007706	0.259875
-38.861636	-2.279861	1.911834	0.007671	0.259874
-39.649085	-2.177590	1.916838	0.007817	0.259646
-39.971977	-2.133604	1.921843	0.007877	0.259563
-39.975697	-2.141745	1.926848	0.007878	0.259514
-40.628006	-2.062463	1.931853	0.008000	0.259294
-40.045192	-2.169246	1.936858	0.007891	0.259289
-40.209386	-2.178297	1.941862	0.007922	0.259071
-41.016345	-2.052204	1.946867	0.008072	0.258955
-40.232457	-2.202641	1.951872	0.007926	0.258911
-40.699767	-2.168105	1.956877	0.008013	0.258629
-40.881925	-2.134581	1.961882	0.008047	0.258631
-41.178116	-2.110926	1.966886	0.008102	0.258461
-41.045175	-2.162924	1.971891	0.008078	0.258305
-40.819844	-2.209958	1.976896	0.008036	0.258271
-41.689737	-2.095118	1.981901	0.008198	0.258027
-41.137109	-2.196801	1.986906	0.008095	0.258020
-41.414885	-2.181672	1.991910	0.008147	0.257821
-42.153380	-2.070515	1.996915	0.008284	0.257691
-41.728518	-2.179116	2.001920	0.008205	0.257514

-42.249067	-2.113551	2.011917	0.008302	0.257350
-42.106314	-2.194984	2.021914	0.008276	0.257037
-41.960547	-2.251287	2.031910	0.008249	0.256869
-42.549601	-2.165063	2.041907	0.008358	0.256750
-42.471416	-2.226348	2.051904	0.008344	0.256484
-42.740857	-2.189709	2.061901	0.008394	0.256414
-43.170283	-2.139205	2.071898	0.008474	0.256257
-43.792083	-2.048771	2.081894	0.008590	0.256129
-43.808665	-2.043247	2.091891	0.008593	0.256142
-43.505415	-2.101316	2.101888	0.008537	0.256126
-43.386308	-2.136359	2.111885	0.008515	0.256050
-43.799991	-2.103826	2.121882	0.008592	0.255807
-43.742845	-2.116150	2.131878	0.008581	0.255796
-43.881237	-2.089423	2.141875	0.008607	0.255804
-43.947380	-2.075806	2.151872	0.008619	0.255813
-43.475885	-2.163965	2.161869	0.008532	0.255799
-43.444483	-2.169611	2.171866	0.008526	0.255799
-43.496481	-2.161118	2.181862	0.008536	0.255793
-43.697489	-2.122961	2.191859	0.008573	0.255801
-43.682311	-2.113801	2.201856	0.008570	0.255868
-44.083353	-1.992424	2.211853	0.008645	0.256142
-43.519687	-2.097058	2.221850	0.008540	0.256130
-43.677677	-2.069382	2.231846	0.008570	0.256123
-43.676372	-2.068809	2.241843	0.008570	0.256127
-43.266079	-2.103507	2.251840	0.008493	0.256353
-43.300845	-2.081499	2.261837	0.008500	0.256441
-43.355374	-2.071517	2.271834	0.008510	0.256441
-43.205864	-2.076708	2.281830	0.008482	0.256565
-42.895265	-2.098598	2.291827	0.008425	0.256760
-43.139842	-2.051706	2.301824	0.008470	0.256773
-42.727831	-2.094171	2.311821	0.008394	0.256955
-42.594121	-2.100527	2.321818	0.008369	0.257056
-43.003717	-2.012161	2.331814	0.008445	0.257134
-42.458565	-2.066202	2.341811	0.008344	0.257388
-42.485609	-2.060113	2.351808	0.008349	0.257394
-42.002418	-2.094773	2.361805	0.008259	0.257693
-41.582828	-2.173983	2.371802	0.008181	0.257676
-41.470002	-2.149728	2.381798	0.008160	0.257927
-41.166154	-2.189301	2.391795	0.008104	0.258015
-41.195845	-2.161562	2.401792	0.008109	0.258140
-40.579698	-2.245020	2.411789	0.007995	0.258300
-40.429325	-2.264563	2.421786	0.007967	0.258343
-40.251810	-2.247943	2.431782	0.007934	0.258617
-40.132651	-2.269886	2.441779	0.007912	0.258615
-39.965557	-2.249464	2.451776	0.007880	0.258899
-39.889344	-2.257048	2.461773	0.007866	0.258934
-40.031365	-2.176956	2.471770	0.007893	0.259237
-39.810181	-2.209965	2.481766	0.007852	0.259277
-39.564470	-2.203624	2.491763	0.007806	0.259561
-39.441759	-2.213754	2.501760	0.007783	0.259629
-39.194890	-2.212016	2.511757	0.007737	0.259889
-39.299128	-2.161955	2.521754	0.007757	0.260061
-38.862480	-2.215271	2.531750	0.007676	0.260206
-39.255108	-2.087284	2.541747	0.007749	0.260520
-39.005663	-2.109728	2.551744	0.007702	0.260648
-38.634413	-2.148268	2.561741	0.007633	0.260808
-38.250920	-2.170799	2.571738	0.007562	0.261070
-38.507604	-2.094580	2.581734	0.007610	0.261233
-38.142076	-2.125464	2.591731	0.007542	0.261430
-37.582948	-2.174006	2.601728	0.007438	0.261724
-37.370013	-2.188499	2.611725	0.007398	0.261858
-37.154435	-2.196473	2.621722	0.007358	0.262030
-36.828250	-2.204536	2.631718	0.007298	0.262313
-37.224769	-2.099691	2.641715	0.007372	0.262493
-36.723398	-2.157274	2.651712	0.007278	0.262678
-36.498453	-2.134913	2.661709	0.007237	0.263026
-36.547221	-2.093008	2.671706	0.007246	0.263208
-36.306665	-2.102343	2.681702	0.007201	0.263396
-36.426443	-2.035041	2.691699	0.007223	0.263646
-35.642500	-2.123305	2.701696	0.007077	0.263944
-35.767342	-2.058576	2.711693	0.007101	0.264174
-35.162132	-2.134033	2.721690	0.006988	0.264363
-34.657443	-2.190718	2.731686	0.006894	0.264555
-34.690082	-2.132725	2.741683	0.006900	0.264840
-34.410030	-2.148995	2.751680	0.006848	0.265029
-33.956812	-2.194049	2.761677	0.006764	0.265233
-34.075149	-2.114232	2.771674	0.006786	0.265550
-33.797449	-2.129152	2.781670	0.006735	0.265744
-33.885594	-2.075169	2.791667	0.006751	0.265950
-33.246446	-2.152653	2.801664	0.006632	0.266161
-33.135969	-2.121464	2.811661	0.006612	0.266439
-32.849501	-2.124290	2.821658	0.006558	0.266706
-32.319994	-2.186220	2.831654	0.006460	0.266893
-32.304786	-2.155501	2.841651	0.006457	0.267074
-32.494689	-2.060823	2.851648	0.006492	0.267399
-32.254431	-2.057264	2.861645	0.006448	0.267655
-31.961869	-2.063344	2.871642	0.006393	0.267909
-31.830218	-2.041960	2.881638	0.006369	0.268154
-31.500240	-2.062074	2.891635	0.006308	0.268368
-30.932538	-2.112354	2.901632	0.006202	0.268654
-30.620498	-2.123278	2.911629	0.006144	0.268900
-30.783817	-2.048649	2.921626	0.006174	0.269142
-30.511681	-2.051730	2.931622	0.006124	0.269391
-30.506267	-2.010723	2.941619	0.006123	0.269616
-29.814378	-2.080095	2.951616	0.005994	0.269919
-29.828762	-2.029215	2.961613	0.005997	0.270177
-29.289023	-2.078615	2.971610	0.005897	0.270438
-29.071893	-2.076491	2.981606	0.005856	0.270660
-28.793314	-2.096209	2.991603	0.005804	0.270825
-28.650895	-2.061679	3.001600	0.005778	0.271148
-28.546158	-2.037165	3.011597	0.005759	0.271380
-28.330435	-2.027814	3.021594	0.005718	0.271639
-28.212193	-2.003109	3.031590	0.005696	0.271884
-27.690925	-2.057014	3.041587	0.005600	0.272102
-27.349056	-2.061355	3.051584	0.005536	0.272409
-27.329921	-2.017206	3.061581	0.005532	0.272661
-27.191080	-1.990070	3.071578	0.005507	0.272939
-26.909761	-1.995463	3.081574	0.005454	0.273181
-26.538041	-2.022153	3.091571	0.005385	0.273398
-25.961387	-2.076049	3.101568	0.005278	0.273667
-25.691256	-2.075939	3.111565	0.005228	0.273927
-25.380707	-2.086258	3.121562	0.005170	0.274170
-25.119787	-2.095286	3.131558	0.005122	0.274373
-24.618394	-2.145935	3.141555	0.005028	0.274586
-24.516131	-2.109124	3.151552	0.005009	0.274878
-24.401510	-2.089783	3.161549	0.004988	0.275089
-24.099185	-2.102035	3.171546	0.004932	0.275313
-24.120719	-2.045695	3.181542	0.004936	0.275588
-23.922328	-2.036102	3.191539	0.004899	0.275828
-23.803708	-2.012830	3.201536	0.004877	0.276063
-23.633358	-1.997111	3.211533	0.004845	0.276307
-23.264919	-2.016626	3.221530	0.004777	0.276555
-23.122234	-1.993278	3.231526	0.004750	0.276813
-22.914546	-1.974936	3.241523	0.004712	0.277106
-22.434933	-2.014337	3.251520	0.004623	0.277355
-22.055517	-2.039127	3.261517	0.004552	0.277585
-21.336046	-2.132734	3.271514	0.004418	0.277779
-21.460064	-2.057069	3.281510	0.004441	0.278055
-20.720454	-2.143964	3.291507	0.004304	0.278302
-21.010166	-2.050231	3.301504	0.004358	0.278516
-20.486721	-2.105085	3.311501	0.004260	0.278725
-20.183385	-2.112901	3.321498	0.004204	0.278970
-19.997159	-2.092241	3.331494	0.004169	0.279252
-19.788940	-2.092330	3.341491	0.004131	0.279448
-19.560572	-2.093369	3.351488	0.004088	0.279657
-19.194139	-2.107775	3.361485	0.004020	0.279927
-19.209766	-2.051680	3.371482	0.004023	0.280202
-19.002924	-2.043660	3.381478	0.003985	0.280437
-18.160263	-2.164079	3.391475	0.003828	0.280606
-18.326275	-2.094008	3.401472	0.003859	0.280811
-18.092773	-2.082636	3.411469	0.003815	0.281088
-17.737724	-2.106301	3.421466	0.003749	0.281298
-17.800520	-2.052855	3.431462	0.003761	0.281514
-17.177911	-2.114492	3.441459	0.003645	0.281778
-17.152721	-2.071822	3.451456	0.003641	0.282021
-16.528367	-2.147815	3.461453	0.003524	0.282213
-16.312774	-2.147688	3.471450	0.003484	0.282414
-15.864625	-2.176253	3.481446	0.003401	0.282685
-15.429365	-2.211390	3.491443	0.003320	0.282910
-15.019838	-2.259707	3.501440	0.003244	0.283043
-14.974659	-2.215149	3.511437	0.003236	0.283312
-14.939110	-2.178243	3.521434	0.003229	0.283533
-14.690644	-2.189820	3.531430	0.003183	0.283704
-14.294877	-2.217258	3.541427	0.003109	0.283931
-14.116433	-2.195539	3.551424	0.003076	0.284207
-13.829927	-2.212991	3.561421	0.003023	0.284383
-13.446020	-2.245721	3.571418	0.002951	0.284571
-13.317343	-2.211354	3.581414	0.002928	0.284864
-12.730986	-2.290893	3.591411	0.002819	0.285001
-12.675055	-2.263207	3.601408	0.002808	0.285193
-12.214836	-2.285074	3.611405	0.002723	0.285506
-12.284283	-2.246542	3.621402	0.002736	0.285637
-12.056043	-2.255785	3.631398	0.002693	0.285800
-11.780737	-2.246492	3.641395	0.002642	0.286100
-11.448090	-2.278733	3.651392	0.002580	0.286242
-11.258898	-2.277216	3.661389	0.002545	0.286423
-11.225833	-2.215453	3.671386	0.002539	0.286765
-10.698996	-2.280138	3.681382	0.002441	0.286922
-10.790826	-2.229933	3.691379	0.002458	0.287090
-10.396699	-2.243961	3.701376	0.002385	0.287380
-9.856065	-2.299843	3.711373	0.002284	0.287593
-9.655663	-2.303898	3.721370	0.002247	0.287756
-9.174839	-2.338881	3.731366	0.002158	0.288019
-9.030616	-2.327831	3.741363	0.002131	0.288206
-8.944340	-2.313673	3.751360	0.002115	0.288355
-8.775869	-2.287569	3.761357	0.002083	0.288639
-8.574083	-2.282278	3.771354	0.002046	0.288849
-8.516556	-2.253548	3.781350	0.002035	0.289045
-8.361959	-2.231223	3.791347	0.002007	0.289297
-8.322591	-2.185635	3.801344	0.001999	0.289561
-8.056612	-2.190696	3.811341	0.001950	0.289777
-7.901955	-2.172963	3.821338	0.001921	0.290005
-7.299498	-2.235871	3.831334	0.001809	0.290237
-7.164749	-2.199330	3.841331	0.001784	0.290541
-6.685602	-2.253296	3.851328	0.001695	0.290706
-6.416865	-2.271672	3.861325	0.001645	0.290857
-6.279627	-2.238754	3.871322	0.001619	0.291144
-6.059717	-2.235602	3.881318	0.001579	0.291358
-6.117273	-2.179642	3.891315	0.001589	0.291584
-5.655106	-2.221300	3.901312	0.001503	0.291793
-5.304886	-2.227437	3.911309	0.001438	0.292078
-4.999515	-2.241487	3.921306	0.001382	0.292283
-4.796678	-2.240487	3.931302	0.001344	0.292470
-4.425200	-2.260770	3.941299	0.001275	0.292703
-4.280082	-2.230816	3.951296	0.001248	0.292981
-4.275700	-2.191961	3.961293	0.001247	0.293177
-3.967435	-2.208359	3.971290	0.001190	0.293372
-3.689429	-2.205134	3.981286	0.001138	0.293637
-3.769048	-2.138173	3.991283	0.001153	0.293895
-3.524071	-2.135603	4.001280	0.001107	0.294126
-3.439380	-2.102387	4.011277	0.001092	0.294365
-3.246946	-2.091376	4.021274	0.001056	0.294590
-3.518811	-1.974177	4.031270	0.001107	0.294923
-3.366578	-1.944333	4.041267	0.001078	0.295204
-2.594913	-2.031310	4.051264	0.000935	0.295465
-2.265450	-2.046417	4.061261	0.000873	0.295684
-2.656889	-1.921807	4.071258	0.000946	0.295945
-2.642991	-1.866208	4.081254	0.000944	0.296229
-2.593352	-1.814447	4.091251	0.000935	0.296525
-2.417121	-1.780523	4.101248	0.000902	0.296846
-1.827763	-1.834928	4.111245	0.000792	0.297103
-1.657146	-1.804822	4.121242	0.000761	0.297400
-1.439714	-1.782298	4.131238	0.000720	0.297701
-1.512690	-1.698443	4.141235	0.000734	0.298044
-1.754529	-1.595167	4.151232	0.000779	0.298331
-1.162770	-1.637741	4.161229	0.000669	0.298646
-0.943288	-1.614396	4.171226	0.000628	0.298952
-1.069953	-1.517723	4.181222	0.000651	0.299308
-0.988675	-1.467822	4.191219	0.000636	0.299620
-0.768865	-1.436245	4.201216	0.000596	0.299965
-0.411835	-1.430901	4.211213	0.000529	0.300303
-0.708420	-1.304364	4.221210	0.000584	0.300652
-0.879585	-1.206666	4.231206	0.000616	0.300972
-0.872998	-1.132643	4.241203	0.000615	0.301333
-0.841040	-1.055393	4.251200	0.000609	0.301731
-0.601733	-1.015052	4.261197	0.000565	0.302133
-0.468274	-0.956487	4.271194	0.000540	0.302529
-0.007981	-0.960315	4.281190	0.000454	0.302910
-0.323628	-0.818299	4.291187	0.000513	0.303314
-0.350347	-0.721387	4.301184	0.000518	0.303752
-0.515830	-0.602860	4.311181	0.000549	0.304173
-0.019223	-0.603419	4.321178	0.000456	0.304599
0.058043	-0.523913	4.331174	0.000442	0.305042
0.190442	-0.456676	4.341171	0.000417	0.305475
0.231203	-0.371650	4.351168	0.000410	0.305912
0.147644	-0.266687	4.361165	0.000425	0.306336
0.226127	-0.170508	4.371162	0.000411	0.306857
0.113254	-0.059141	4.381158	0.000432	0.307285
0.000000	0.073924	4.391155	0.000453	0.307813

-0.294415	0.402292	4.396160	0.000508	0.309103
0.004345	0.897513	4.401165	0.000452	0.311664
-0.125299	1.762123	4.406170	0.000475	0.315544
-0.320097	2.924016	4.411174	0.000511	0.320668
-0.016187	4.277529	4.416179	0.000453	0.326963
1.096662	5.775481	4.421184	0.000245	0.334401
0.946053	7.813249	4.426189	0.000272	0.342989
0.635001	10.189248	4.431194	0.000328	0.352638
0.941887	12.749107	4.436198	0.000270	0.363211
1.184269	15.635633	4.441203	0.000223	0.374703
1.713018	18.795758	4.446208	0.000122	0.387071
1.969199	22.342988	4.451213	0.000072	0.400279
2.663743	26.145061	4.456218	-0.000060	0.414233
2.745059	30.414223	4.461222	-0.000077	0.428934
2.612445	35.054232	4.466227	-0.000056	0.444232
2.935059	39.967416	4.471232	-0.000119	0.460138
3.543825	45.163220	4.476237	-0.000236	0.476529
3.742572	50.780548	4.481242	-0.000276	0.493394
3.822987	56.772140	4.486246	-0.000295	0.510702
4.388115	62.981591	4.491251	-0.000404	0.528279
4.437354	69.622879	4.496256	-0.000418	0.546187
4.818196	76.498539	4.501261	-0.000493	0.564281
5.369302	83.650852	4.506266	-0.000600	0.582576
5.395923	91.187113	4.511270	-0.000610	0.601011
5.767783	98.911176	4.516275	-0.000684	0.619480
10.056034	106.211772	4.521280	-0.001488	0.638045
10.925603	114.394606	4.526285	-0.001655	0.656677
11.409752	122.862628	4.531290	-0.001751	0.675258
13.379772	131.248336	4.536294	-0.002123	0.693722
13.902792	140.094536	4.541299	-0.002226	0.712117
15.020099	148.984601	4.546304	-0.002440	0.730345
15.801230	158.089697	4.551309	-0.002591	0.748427
16.657231	167.291309	4.556314	-0.002756	0.766290
17.368528	176.629001	4.561318	-0.002895	0.783949
18.613353	185.946390	4.566323	-0.003133	0.801351
20.635276	195.221742	4.571328	-0.003515	0.818552
21.659710	204.742574	4.576333	-0.003712	0.835516
22.151897	214.379533	4.581338	-0.003810	0.852180
23.730386	223.857319	4.586342	-0.004110	0.868578
24.538151	233.487167	4.591347	-0.004267	0.884697
25.415399	243.119302	4.596352	-0.004436	0.900550
26.259395	252.751389	4.601357	-0.004600	0.916119
26.994729	262.371803	4.606362	-0.004743	0.931379
27.782721	271.980876	4.611366	-0.004896	0.946390
28.292558	281.594084	4.616371	-0.004997	0.961099
29.589454	291.041871	4.621376	-0.005244	0.975544
30.364222	300.566914	4.626381	-0.005395	0.989757
31.510385	309.957249	4.631386	-0.005614	1.003668
32.998009	319.259739	4.636390	-0.005897	1.017347
34.641291	328.500477	4.641395	-0.006209	1.030795
35.628321	337.820618	4.646400	-0.006399	1.044021
36.268011	347.175300	4.651405	-0.006524	1.057046
37.029610	356.452732	4.656410	-0.006672	1.069836
38.371294	365.561191	4.661414	-0.006928	1.082383
38.864921	374.792573	4.666419	-0.007026	1.094754
39.414025	383.956014	4.671424	-0.007134	1.106911
40.331158	392.991744	4.676429	-0.007311	1.118852
42.331788	401.810788	4.681434	-0.007689	1.130627
44.108676	410.684128	4.686438	-0.008025	1.142300
44.497611	419.774346	4.691443	-0.008104	1.153827
45.420521	428.675308	4.696448	-0.008281	1.165119
46.070013	437.596540	4.701453	-0.008408	1.176270
46.297781	446.542923	4.706458	-0.008456	1.187258
47.041887	455.358082	4.711462	-0.008600	1.198093
47.571601	464.153769	4.716467	-0.008705	1.208764
48.537617	472.859174	4.721472	-0.008890	1.219322
49.100211	481.620612	4.726477	-0.009001	1.229774
49.672256	490.309345	4.731482	-0.009113	1.240056
50.616967	498.932419	4.736486	-0.009294	1.250249
51.624507	507.516151	4.741491	-0.009488	1.260326
52.440425	516.128269	4.746496	-0.009645	1.270319
52.740585	524.775424	4.751501	-0.009706	1.280174
53.511507	533.324220	4.756506	-0.009856	1.289933
54.292676	541.879335	4.761510	-0.010007	1.299627
55.182984	550.396317	4.766515	-0.010178	1.309227
55.719325	558.986497	4.771520	-0.010283	1.318772
56.692769	567.399516	4.776525	-0.010470	1.328135
57.908597	575.793268	4.781530	-0.010702	1.337455
58.458469	584.291754	4.786534	-0.010810	1.346702
58.733645	592.810991	4.791539	-0.010866	1.355860
59.935282	601.151566	4.796544	-0.011096	1.364931
59.697834	609.749644	4.801549	-0.011057	1.373959
59.797347	618.228548	4.806554	-0.011081	1.382863
60.564121	626.598149	4.811558	-0.011229	1.391712
61.018938	634.968023	4.816563	-0.011319	1.400451
61.760866	643.323676	4.821568	-0.011463	1.409170
62.880061	651.597580	4.826573	-0.011677	1.417816
63.367236	659.981149	4.831578	-0.011773	1.426414
63.775448	668.380467	4.836582	-0.011854	1.434963
64.432025	676.678951	4.841587	-0.011982	1.443401
64.744266	685.078145	4.846592	-0.012045	1.451833
65.271279	693.417951	4.851597	-0.012149	1.460193
66.271189	701.663024	4.856602	-0.012340	1.468489
66.757590	710.022817	4.861606	-0.012436	1.476767
67.219179	718.299047	4.866611	-0.012528	1.484913
67.875809	726.603169	4.871616	-0.012655	1.493073
68.365770	734.898532	4.876621	-0.012752	1.501154
68.757832	743.218619	4.881626	-0.012830	1.509199
70.836832	751.248361	4.886630	-0.013223	1.517188
71.682164	759.499458	4.891635	-0.013385	1.525153
72.659328	767.763087	4.896640	-0.013573	1.533108
72.872891	776.123552	4.901645	-0.013618	1.540996
73.685762	784.384282	4.906650	-0.013774	1.548841
74.080690	792.707174	4.911654	-0.013853	1.556642
74.797483	800.919925	4.916659	-0.013992	1.564350
75.582606	809.161356	4.921664	-0.014144	1.572056
76.037932	817.439845	4.926669	-0.014234	1.579710
76.295552	825.746578	4.931674	-0.014287	1.587323
76.976611	833.974065	4.936678	-0.014419	1.594890
77.957138	842.119111	4.941683	-0.014607	1.602390
79.106898	850.283077	4.946688	-0.014826	1.609896
79.695922	858.548133	4.951693	-0.014941	1.617376
80.036558	866.817400	4.956698	-0.015010	1.624791
80.629805	875.099752	4.961702	-0.015126	1.632218
80.828769	883.351623	4.966707	-0.015168	1.639530
81.399238	891.555044	4.971712	-0.015280	1.646819
81.947632	899.760932	4.976717	-0.015387	1.654074
82.421012	907.952608	4.981722	-0.015481	1.661275
83.077805	916.136933	4.986726	-0.015608	1.668463
83.555854	924.339920	4.991731	-0.015703	1.675612
83.598842	932.623067	4.996736	-0.015716	1.682740
83.623781	940.873772	5.001741	-0.015726	1.689808
84.019929	949.055869	5.006746	-0.015805	1.696837
84.430838	957.236315	5.011750	-0.015887	1.703839
84.999433	965.404319	5.016755	-0.015998	1.710822
85.674838	973.557526	5.021760	-0.016129	1.717778
86.024280	981.726743	5.026765	-0.016200	1.724676
87.112307	989.796280	5.031770	-0.016407	1.731560
88.140902	997.914645	5.036774	-0.016604	1.738450
88.969170	1006.039276	5.041779	-0.016764	1.745291
89.449200	1014.292038	5.046784	-0.016858	1.752166
90.126272	1022.442446	5.051789	-0.016990	1.758955
90.793082	1030.605476	5.056794	-0.017119	1.765727
91.876335	1038.730869	5.061798	-0.017326	1.772495
92.213652	1046.958496	5.066803	-0.017394	1.779225
92.654328	1055.146882	5.071808	-0.017482	1.785912
93.288326	1063.339625	5.076813	-0.017605	1.792601
93.551247	1071.529677	5.081818	-0.017659	1.799216
94.447609	1079.605906	5.086822	-0.017831	1.805795
94.758872	1087.805579	5.091827	-0.017895	1.812375
95.454329	1095.931622	5.096832	-0.018029	1.818921
95.879141	1104.105019	5.101837	-0.018114	1.825447
96.804884	1112.190892	5.106842	-0.018291	1.831941
97.166393	1120.419275	5.111846	-0.018364	1.838456
97.521266	1128.546747	5.116851	-0.018435	1.844869
98.341041	1136.665353	5.121856	-0.018593	1.851307
99.041938	1144.797736	5.126861	-0.018729	1.857720
99.142409	1153.008521	5.131866	-0.018753	1.864099
99.650450	1161.166062	5.136870	-0.018853	1.870464
100.125079	1169.281485	5.141875	-0.018946	1.876771
101.245893	1177.307945	5.146880	-0.019160	1.883065
101.951016	1185.430481	5.151885	-0.019297	1.889361
102.392235	1193.602164	5.156890	-0.019384	1.895644
103.252832	1201.709738	5.161894	-0.019550	1.901905
103.530227	1209.901959	5.166899	-0.019607	1.908142
104.231526	1218.011104	5.171904	-0.019743	1.914345
105.086762	1226.080427	5.176909	-0.019907	1.920516
105.699315	1234.213670	5.181914	-0.020026	1.926686
106.204670	1242.397723	5.186918	-0.020126	1.932863
106.490323	1250.554572	5.191923	-0.020184	1.938975
106.887352	1258.686958	5.196928	-0.020263	1.945062
107.173880	1266.868597	5.201933	-0.020322	1.951153
107.270835	1275.013776	5.206938	-0.020345	1.957178
108.287729	1283.047153	5.211942	-0.020540	1.963204
108.721400	1291.159573	5.216947	-0.020626	1.969205
109.464094	1299.240334	5.221952	-0.020769	1.975198
110.184967	1307.329626	5.226957	-0.020909	1.981177
110.542107	1315.475803	5.231962	-0.020981	1.987139
111.283459	1323.571284	5.236966	-0.021124	1.993088
111.445187	1331.748624	5.241971	-0.021159	1.999016
112.526271	1339.743406	5.246976	-0.021366	2.004893
112.539399	1347.972324	5.251981	-0.021374	2.010807
113.346485	1356.014614	5.256986	-0.021529	2.016655
113.850763	1364.149050	5.261990	-0.021628	2.022519
114.135623	1372.287144	5.266995	-0.021686	2.028345
114.512933	1380.441599	5.272000	-0.021762	2.034176
114.282660	1388.640238	5.277005	-0.021724	2.039958
114.658856	1396.697225	5.282010	-0.021800	2.045687
115.262559	1404.782444	5.287014	-0.021917	2.051443
115.839957	1412.852902	5.292019	-0.022030	2.057170
116.516026	1420.924913	5.297024	-0.022161	2.062892
117.025235	1429.046627	5.302029	-0.022261	2.068616
117.443793	1437.148880	5.307034	-0.022344	2.074301
118.052378	1445.220015	5.312038	-0.022463	2.079968
118.262889	1453.354018	5.317043	-0.022507	2.085622
119.320610	1461.367605	5.322048	-0.022710	2.091264
119.816735	1469.483054	5.327053	-0.022807	2.096903
120.127195	1477.636868	5.332058	-0.022870	2.102536
120.823398	1485.723648	5.337062	-0.023005	2.108145
121.174642	1493.872090	5.342067	-0.023076	2.113748
121.521718	1501.968502	5.347072	-0.023146	2.119299
121.969712	1510.016167	5.352077	-0.023234	2.124813
122.383650	1518.096479	5.357082	-0.023317	2.130332
123.019595	1526.180123	5.362086	-0.023440	2.135859
123.270280	1534.305076	5.367091	-0.023492	2.141363
123.486517	1542.463073	5.372096	-0.023538	2.146872
124.407710	1550.467685	5.377101	-0.023714	2.152331
125.008570	1558.534199	5.382106	-0.023831	2.157787
125.314415	1566.659459	5.387110	-0.023894	2.163240
125.395895	1574.811310	5.392115	-0.023914	2.168676
125.401403	1582.977376	5.397120	-0.023920	2.174100
125.889727	1591.029321	5.402125	-0.024017	2.179481
126.169904	1599.088898	5.407130	-0.024074	2.184833
126.832426	1607.135347	5.412134	-0.024202	2.190200
127.109061	1615.222700	5.417139	-0.024259	2.195545
127.697225	1623.297407	5.422144	-0.024374	2.200897
128.367532	1631.320388	5.427149	-0.024504	2.206209
129.201867	1639.373260	5.432154	-0.024665	2.211544
129.833371	1647.445857	5.437158	-0.024787	2.216859
130.206083	1655.549600	5.442163	-0.024862	2.222159
130.948620	1663.617198	5.447168	-0.025005	2.227455
131.030503	1671.792529	5.452173	-0.025026	2.232749
131.527250	1679.855335	5.457178	-0.025124	2.237995
132.038553	1687.943889	5.462182	-0.025224	2.243246
132.301318	1696.045501	5.467187	-0.025278	2.248472
132.657532	1704.151123	5.472192	-0.025350	2.253695
133.620178	1712.138919	5.477197	-0.025534	2.258886
133.798745	1720.243529	5.482202	-0.025573	2.264069
133.335910	1728.550401	5.487206	-0.025492	2.269312
133.932988	1736.567019	5.492211	-0.025608	2.274453
133.922791	1744.661983	5.497216	-0.025612	2.279578
134.710258	1752.609729	5.502221	-0.025763	2.284668
134.911315	1760.718322	5.507226	-0.025806	2.289797
135.577093	1768.773938	5.512230	-0.025935	2.294922
135.841941	1776.845711	5.517235	-0.025990	2.300010
136.080937	1784.934386	5.522240	-0.026040	2.305095
136.665250	1792.960469	5.527245	-0.026154	2.310160
137.329221	1800.978575	5.532250	-0.026282	2.315216
137.686280	1809.093309	5.537254	-0.026354	2.320294
137.941498	1817.154460	5.542259	-0.026407	2.325319
138.364056	1825.257478	5.547264	-0.026491	2.330373
138.814424	1833.307573	5.552269	-0.026580	2.335386
139.067811	1841.394108	5.557274	-0.026632	2.340394
139.285306	1849.510667	5.562278	-0.026678	2.345406
139.963185	1857.529563	5.567283	-0.026809	2.350387
140.408508	1865.599130	5.572288	-0.026898	2.355368
140.484307	1873.719966	5.577293	-0.026917	2.360339
141.194210	1881.683810	5.582298	-0.027054	2.365257
141.657389	1889.808781	5.587302	-0.027146	2.370242
142.259457	1897.825904	5.592307	-0.027263	2.375162
142.758270	1905.927375	5.597312	-0.027361	2.380115
143.260785	1913.996497	5.602317	-0.027460	2.385038
143.808295	1922.054577	5.607322	-0.027567	2.389947
144.090430	1930.153643	5.612326	-0.027625	2.394850
144.223361	1938.246671	5.617331	-0.027655	2.399727
144.804864	1946.248428	5.622336	-0.027768	2.404575
145.086562	1954.360125	5.627341	-0.027826	2.409455
145.026946	1962.494641	5.632346	-0.027820	2.414312
145.622830	1970.549308	5.637350	-0.027936	2.419163
146.211845	1978.523284	5.642355	-0.028051	2.423956
146.848180	1986.592889	5.647360	-0.028175	2.428800
147.156072	1994.728246	5.652365	-0.028237	2.433648
147.489844	2002.774659	5.657370	-0.028305	2.438435
148.134513	2010.805948	5.662374	-0.028430	2.443227
148.577417	2018.848069	5.667379	-0.028518	2.448001
149.099301	2026.907436	5.672384	-0.028620	2.452782
149.650459	2034.948670	5.677389	-0.028728	2.457545
150.396004	2042.938914	5.682394	-0.028872	2.462284
150.019716	2051.189413	5.687398	-0.028807	2.467080
150.316031	2059.253025	5.692403	-0.028868	2.471808
150.677044	2067.297234	5.697408	-0.028940	2.476522
150.894933	2075.349961	5.702413	-0.028986	2.481220
150.921058	2083.441572	5.707418	-0.028996	2.485917
151.230608	2091.526060	5.712422	-0.029059	2.490623
151.569557	2099.553020	5.717427	-0.029127	2.495289
152.000595	2107.609502	5.722432	-0.029212	2.499970
152.556811	2115.613001	5.727437	-0.029321	2.504621
152.818457	2123.690101	5.732442	-0.029375	2.509284
153.030201	2131.795404	5.737446	-0.029420	2.513950
153.457898	2139.803655	5.742451	-0.029505	2.518568
153.662059	2147.867529	5.747456	-0.029548	2.523193
154.027183	2155.931039	5.752461	-0.029621	2.527821
155.078685	2163.880242	5.757466	-0.029822	2.532425
155.437995	2171.988336	5.762470	-0.029894	2.537061
155.638896	2180.077880	5.767475	-0.029937	2.541666
157.004776	2187.997490	5.772480	-0.030196	2.546251
157.374199	2196.131707	5.777485	-0.030270	2.550877
157.670068	2204.187904	5.782490	-0.030331	2.555445
158.186998	2212.255445	5.787494	-0.030432	2.560027
158.837643	2220.240983	5.792499	-0.030558	2.564564
159.230080	2228.345474	5.797504	-0.030637	2.569141
159.409857	2236.459633	5.802509	-0.030675	2.573701
159.571526	2244.553168	5.807514	-0.030711	2.578239
160.051340	2252.588587	5.812518	-0.030805	2.582760
159.688596	2260.760669	5.817523	-0.030743	2.587289
160.668348	2268.767747	5.822528	-0.030931	2.591813
161.149600	2276.860167	5.827533	-0.031025	2.596341
160.981771	2284.961391	5.832538	-0.030999	2.600821
161.563317	2292.928650	5.837542	-0.031113	2.605271
161.795617	2300.965606	5.842547	-0.031161	2.609728
162.331008	2308.979599	5.847552	-0.031266	2.614186
162.705893	2317.005272	5.852557	-0.031341	2.618631
162.975053	2325.057457	5.857562	-0.031397	2.623076
163.462541	2333.119868	5.862566	-0.031493	2.627533
164.015961	2341.117622	5.867571	-0.031601	2.631952
164.367307	2349.187996	5.872576	-0.031671	2.636390
165.022504	2357.205277	5.877581	-0.031799	2.640812
165.269114	2365.244622	5.882586	-0.031850	2.645210
165.633479	2373.356719	5.887590	-0.031923	2.649649
166.368659	2381.359178	5.892595	-0.032065	2.654046
166.649278	2389.453614	5.897600	-0.032122	2.658454
166.834652	2397.540498	5.902605	-0.032162	2.662845
167.374852	2405.553861	5.907610	-0.032268	2.667212
168.073248	2413.609323	5.912614	-0.032403	2.671606
168.050938	2421.710556	5.917619	-0.032404	2.675969
168.450721	2429.714675	5.922624	-0.032484	2.680300
169.026561	2437.721530	5.927629	-0.032596	2.684638
169.303777	2445.758878	5.932634	-0.032653	2.688965
169.285617	2453.920623	5.937638	-0.032655	2.693332
169.622903	2461.951240	5.942643	-0.032723	2.697645
170.044328	2469.977087	5.947648	-0.032807	2.701955
170.587227	2478.005385	5.952653	-0.032913	2.706266
170.946914	2486.043132	5.957658	-0.032985	2.710564
171.303232	2494.137807	5.962662	-0.033057	2.714885
171.648080	2502.126153	5.967667	-0.033126	2.719142
171.835717	2510.214044	5.972672	-0.033166	2.723434
172.219184	2518.284173	5.977677	-0.033243	2.727723
172.743918	2526.281586	5.982682	-0.033346	2.731976
173.307323	2534.341705	5.987686	-0.033456	2.736258
173.776970	2542.377882	5.992691	-0.033548	2.740514
174.243415	2550.408176	5.997696	-0.033640	2.744760
174.440730	2558.541674	6.002701	-0.033682	2.749037
175.031009	2566.562396	6.007706	-0.033798	2.753273
176.057897	2574.523004	6.012710	-0.033994	2.757497
176.485015	2582.558005	6.017715	-0.034079	2.761717
177.117379	2590.579436	6.022720	-0.034202	2.765936
177.357772	2598.684463	6.027725	-0.034252	2.770167
177.507128	2606.751428	6.032730	-0.034285	2.774367
178.296625	2614.729355	6.037734	-0.034437	2.778553
178.817345	2622.776737	6.042739	-0.034539	2.782753
178.732522	2630.924032	6.047744	-0.034528	2.786961
179.038209	2638.989391	6.052749	-0.034591	2.791143
179.539581	2647.003515	6.057754	-0.034689	2.795305
180.173272	2654.997414	6.062758	-0.034812	2.799459
180.448347	2663.047829	6.067763	-0.034869	2.803613
180.885387	2671.103655	6.072768	-0.034955	2.807774
181.905434	2679.061205	6.077773	-0.035150	2.811913
182.064676	2687.170693	6.082778	-0.035185	2.816072
182.435060	2695.232329	6.087782	-0.035259	2.820213
182.465971	2703.330001	6.092787	-0.035270	2.824346
182.536791	2711.439858	6.097792	-0.035289	2.828482
183.119664	2719.420897	6.102797	-0.035403	2.832576
183.960387	2727.366294	6.107802	-0.035564	2.836661
184.465277	2735.423198	6.112806	-0.035663	2.840777
184.628826	2743.458450	6.117811	-0.035699	2.844856
184.537014	2751.614890	6.122816	-0.035687	2.848976
184.944795	2759.628223	6.127821	-0.035768	2.853046
185.490872	2767.631873	6.132826	-0.035875	2.857114
185.828674	2775.690825	6.137830	-0.035943	2.861192
186.113817	2783.712784	6.142835	-0.036002	2.865242
186.364319	2791.773835	6.147840	-0.036053	2.869304
186.346847	2799.888672	6.152845	-0.036055	2.873372
187.158111	2807.807663	6.157850	-0.036212	2.877383
187.773029	2815.843439	6.162854	-0.036331	2.881436
187.519318	2823.990712	6.167859	-0.036289	2.885489
187.838522	2832.041577	6.172864	-0.036354	2.889521
188.499441	2840.044760	6.177869	-0.036482	2.893543
188.771146	2848.077350	6.182874	-0.036538	2.897552
189.358102	2856.092836	6.187878	-0.036653	2.901565
189.989931	2864.083854	6.192883	-0.036775	2.905562
190.392070	2872.152245	6.197888	-0.036855	2.909579
190.730449	2880.297248	6.202893	-0.036924	2.913625
190.582383	2888.343349	6.207898	-0.036901	2.917589
191.004378	2896.363648	6.212902	-0.036985	2.921567
191.196677	2904.395825	6.217907	-0.037026	2.925533
191.582793	2912.386439	6.222912	-0.037103	2.929483
192.062670	2920.445138	6.227917	-0.037198	2.933466
192.598412	2928.437549	6.232922	-0.037303	2.937415
193.051874	2936.483236	6.237926	-0.037392	2.941379
193.698914	2944.469582	6.242931	-0.037518	2.945320
194.088818	2952.534190	6.247936	-0.037596	2.949279
194.241906	2960.620401	6.252941	-0.037629	2.953232
194.486689	2968.683784	6.257946	-0.037680	2.957172
195.496463	2976.616194	6.262950	-0.037873	2.961084
195.983439	2984.633916	6.267955	-0.037969	2.965005
196.084705	2992.739203	6.272960	-0.037993	2.968942
196.657529	3000.769346	6.277965	-0.038105	2.972863
196.474045	3008.908428	6.282970	-0.038076	2.976791
196.937172	3016.924931	6.287974	-0.038168	2.980689
197.277416	3024.922711	6.292979	-0.038236	2.984566
198.141896	3032.907040	6.297984	-0.038402	2.988459
198.799398	3040.954352	6.302989	-0.038530	2.992366
198.910883	3049.010676	6.307994	-0.038556	2.996245
199.279019	3057.055876	6.312998	-0.038630	3.000126
199.462462	3065.084522	6.318003	-0.038669	3.003984
199.444639	3073.183566	6.323008	-0.038671	3.007861
199.834003	3081.237929	6.328013	-0.038749	3.011732
200.308769	3089.252579	6.333018	-0.038842	3.015584
201.017171	3097.237220	6.338022	-0.038979	3.019428
200.848517	3105.349579	6.343027	-0.038953	3.023284
201.801470	3113.288623	6.348032	-0.039136	3.027108
201.985253	3121.392367	6.353037	-0.039175	3.030968
202.248778	3129.407950	6.358042	-0.039230	3.034785
202.977076	3137.378312	6.363046	-0.039370	3.038598
203.548865	3145.408501	6.368051	-0.039482	3.042427
203.700163	3153.515626	6.373056	-0.039515	3.046267
204.397294	3161.460865	6.378061	-0.039650	3.050052
204.756005	3169.496711	6.383066	-0.039722	3.053859
205.211986	3177.586381	6.388070	-0.039812	3.057691
205.222911	3185.705478	6.393075	-0.039820	3.061510
205.637353	3193.724358	6.398080	-0.039902	3.065297
206.156204	3201.751887	6.403085	-0.040004	3.069088
205.747022	3209.932217	6.408090	-0.039933	3.072902
206.297948	3217.889942	6.413094	-0.040041	3.076652
206.887467	3225.865724	6.418099	-0.040156	3.080409
207.324518	3233.832428	6.423104	-0.040242	3.084149
207.369168	3241.953136	6.428109	-0.040256	3.087938
207.718043	3249.973543	6.433114	-0.040326	3.091689
208.100459	3258.029331	6.438118	-0.040402	3.095454
208.386727	3266.006762	6.443123	-0.040461	3.099174
208.817893	3274.022941	6.448128	-0.040546	3.102914
209.510125	3282.020470	6.453133	-0.040680	3.106653
209.395485	3290.127371	6.458138	-0.040664	3.110400
209.714740	3298.175077	6.463142	-0.040729	3.114135
210.012861	3306.182660	6.468147	-0.040790	3.117847
210.455722	3314.207024	6.473152	-0.040877	3.121568
211.032712	3322.180907	6.478157	-0.040990	3.125268
211.628897	3330.194524	6.483162	-0.041106	3.128983
212.263659	3338.249458	6.488166	-0.041229	3.132713
212.379365	3346.323376	6.493171	-0.041256	3.136424
212.715141	3354.366552	6.498176	-0.041324	3.140127
213.122911	3362.397898	6.503181	-0.041405	3.143823
213.301462	3370.450779	6.508186	-0.041443	3.147514
213.296108	3378.602583	6.513190	-0.041448	3.151238
213.860949	3386.570622	6.518195	-0.041558	3.154899
214.223779	3394.582574	6.523200	-0.041631	3.158567
214.636003	3402.595039	6.528205	-0.041713	3.162233
215.013408	3410.623193	6.533210	-0.041788	3.165900
215.398238	3418.670441	6.538214	-0.041865	3.169572
215.495361	3426.716878	6.543219	-0.041888	3.173226
215.770124	3434.736642	6.548224	-0.041945	3.176872
216.096589	3442.804888	6.553229	-0.042011	3.180538
216.483276	3450.755811	6.558234	-0.042088	3.184149
217.059760	3458.803343	6.563238	-0.042200	3.187808
217.371338	3466.858436	6.568243	-0.042264	3.191454
218.137183	3474.819942	6.573248	-0.042411	3.195074
218.360491	3482.896100	6.578253	-0.042458	3.198718
218.708439	3490.911868	6.583258	-0.042528	3.202336
219.153095	3498.962357	6.588262	-0.042616	3.205969
219.380411	3507.012450	6.593267	-0.042664	3.209589
219.563583	3515.096211	6.598272	-0.042703	3.213218
220.079598	3523.118245	6.603277	-0.042804	3.216829
220.006142	3531.146462	6.608282	-0.042796	3.220413
220.704305	3539.081335	6.613286	-0.042931	3.223985
220.830867	3547.175021	6.618291	-0.042960	3.227600
221.306520	3555.239093	6.623296	-0.043053	3.231212
221.146084	3563.316535	6.628301	-0.043029	3.234798
221.678091	3571.275535	6.633306	-0.043133	3.238358
221.681780	3579.362378	6.638310	-0.043139	3.241948
221.833304	3587.363964	6.643315	-0.043172	3.245502
222.455967	3595.308969	6.648320	-0.043293	3.249047
223.138039	3603.349882	6.653325	-0.043426	3.252633
223.171036	3611.446621	6.658330	-0.043437	3.256213
223.735321	3619.412813	6.663334	-0.043547	3.259753
224.085443	3627.436242	6.668339	-0.043618	3.263305
224.562562	3635.485859	6.673344	-0.043712	3.266871
224.829034	3643.561220	6.678349	-0.043766	3.270435
224.668019	3651.631813	6.683354	-0.043742	3.273976
225.343721	3659.591773	6.688358	-0.043873	3.277498
225.338206	3667.666186	6.693363	-0.043877	3.281039
225.733190	3675.641884	6.698368	-0.043956	3.284549
226.081659	3683.688401	6.703373	-0.044026	3.288084
226.556482	3691.682874	6.708378	-0.044119	3.291598
226.719066	3699.761888	6.713382	-0.044155	3.295132
227.113029	3707.782007	6.718387	-0.044233	3.298647
227.199451	3715.839593	6.723392	-0.044255	3.302161
227.296027	3723.914937	6.728397	-0.044278	3.305680
227.991350	3731.830437	6.733402	-0.044412	3.309149
228.408980	3739.922820	6.738406	-0.044495	3.312680
228.745861	3747.949264	6.743411	-0.044563	3.316176
229.186765	3755.911557	6.748416	-0.044651	3.319644
229.406496	3763.972977	6.753421	-0.044697	3.323143
229.962736	3771.962276	6.758426	-0.044805	3.326620
230.346797	3780.042130	6.763430	-0.044882	3.330126
230.755948	3788.056801	6.768435	-0.044964	3.333600
231.473401	3796.041707	6.773440	-0.045102	3.337071
231.509950	3804.186462	6.778445	-0.045114	3.340580
231.174471	3812.222511	6.783450	-0.045057	3.344024
231.494497	3820.274092	6.788454	-0.045122	3.347497
231.989130	3828.252569	6.793459	-0.045219	3.350941
232.231076	3836.254480	6.798464	-0.045269	3.354382
232.543408	3844.296454	6.803469	-0.045333	3.357839
232.927887	3852.339086	6.808474	-0.045410	3.361296
232.934265	3860.376523	6.813478	-0.045416	3.364733
233.222172	3868.398335	6.818483	-0.045475	3.368170
234.141636	3876.354424	6.823488	-0.045651	3.371599
234.492499	3884.405865	6.828493	-0.045722	3.375043
234.769969	3892.422923	6.833498	-0.045778	3.378467
235.141838	3900.498097	6.838502	-0.045853	3.381916
235.362393	3908.496262	6.843507	-0.045899	3.385323
235.545390	3916.596339	6.848512	-0.045938	3.388768
235.883204	3924.663457	6.853517	-0.046007	3.392201
235.936660	3932.700628	6.858522	-0.046022	3.395608
236.536398	3940.642329	6.863526	-0.046139	3.398991
237.036781	3948.609581	6.868531	-0.046237	3.402377
237.461281	3956.640288	6.873536	-0.046321	3.405784
237.566348	3964.730082	6.878541	-0.046346	3.409201
237.925697	3972.767214	6.883546	-0.046418	3.412601
238.641651	3980.746029	6.888550	-0.046556	3.415987
238.751968	3988.802778	6.893555	-0.046582	3.419380
239.187049	3996.782269	6.898560	-0.046668	3.422748
239.420685	4004.882734	6.903565	-0.046717	3.426157
240.048816	4012.863740	6.908570	-0.046839	3.429526
240.784043	4020.852891	6.913574	-0.046981	3.432900
240.722000	4028.947350	6.918579	-0.046975	3.436285
241.390362	4036.908315	6.923584	-0.047105	3.439637
242.362628	4044.883545	6.928589	-0.047291	3.443003
242.307362	4052.988070	6.933594	-0.047286	3.446383
242.668846	4061.028639	6.938598	-0.047358	3.449747
242.815140	4069.091223	6.943603	-0.047391	3.453110
242.876320	4077.144720	6.948608	-0.047407	3.456463
243.294963	4085.164725	6.953613	-0.047490	3.459811
244.135244	4093.094261	6.958618	-0.047652	3.463133
244.337461	4101.226955	6.963622	-0.047695	3.466514
244.707540	4109.237207	6.968627	-0.047769	3.469846
244.837432	4117.247697	6.973632	-0.047798	3.473167
244.812516	4125.341144	6.978637	-0.047799	3.476515
244.983125	4133.298086	6.983642	-0.047836	3.479809
245.403636	4141.308313	6.988646	-0.047919	3.483130
245.588270	4149.367331	6.993651	-0.047959	3.486460
245.930264	4157.392712	6.998656	-0.048028	3.489778
246.030165	4165.453631	7.003661	-0.048052	3.493100
246.579583	4173.423333	7.008666	-0.048159	3.496396
247.049699	4181.445145	7.013670	-0.048252	3.499708
247.475030	4189.418231	7.018675	-0.048336	3.502994
247.894159	4197.501559	7.023680	-0.048419	3.506323
248.268866	4205.529198	7.028685	-0.048494	3.509624
248.407750	4213.575554	7.033690	-0.048525	3.512922
248.915193	4221.599007	7.038694	-0.048625	3.516220
249.668881	4229.538270	7.043699	-0.048771	3.519488
250.008607	4237.590387	7.048704	-0.048839	3.522785
250.170172	4245.683281	7.053709	-0.048874	3.526090
250.536394	4253.672834	7.058714	-0.048948	3.529357
251.093880	4261.732605	7.063718	-0.049057	3.532655
251.157866	4269.763161	7.068723	-0.049074	3.535922
251.651950	4277.741008	7.073728	-0.049171	3.539179
252.208463	4285.779340	7.078733	-0.049280	3.542459
252.384082	4293.809248	7.083738	-0.049318	3.545721
252.708893	4301.863713	7.088742	-0.049383	3.548994
253.027308	4309.933979	7.093747	-0.049448	3.552270
253.360281	4317.962074	7.098752	-0.049515	3.555526
253.855926	4325.905667	7.103757	-0.049613	3.558751
254.138821	4333.922386	7.108762	-0.049670	3.561995
254.259106	4341.960422	7.113766	-0.049698	3.565240
254.318103	4350.008924	7.118771	-0.049714	3.568485
254.496350	4358.058900	7.123776	-0.049753	3.571730
254.883261	4366.065647	7.128781	-0.049830	3.574962
255.230794	4374.035354	7.133786	-0.049900	3.578174
255.373635	4382.141303	7.138790	-0.049932	3.581433
255.844306	4390.086947	7.143795	-0.050024	3.584633
256.115076	4398.139756	7.148800	-0.050080	3.587868
256.397472	4406.238892	7.153805	-0.050138	3.591119
256.568627	4414.196768	7.158810	-0.050175	3.594306
257.320777	4422.156423	7.163814	-0.050320	3.597509
257.486314	4430.222256	7.168819	-0.050356	3.600734
257.871816	4438.189984	7.173824	-0.050433	3.603924
257.747769	4446.349613	7.178829	-0.050415	3.607172
258.278650	4454.293779	7.183834	-0.050519	3.610350
258.259673	4462.396738	7.188838	-0.050521	3.613573
258.875974	4470.359404	7.193843	-0.050641	3.616756
259.133537	4478.382890	7.198848	-0.050694	3.619949
259.532988	4486.392311	7.203853	-0.050773	3.623138
260.032881	4494.439562	7.208858	-0.050872	3.626343
260.403335	4502.492426	7.213862	-0.050946	3.629542
260.839334	4510.501302	7.218867	-0.051032	3.632724
260.898803	4518.549843	7.223872	-0.051049	3.635907
261.525152	4526.508134	7.228877	-0.051170	3.639068
261.563905	4534.577133	7.233882	-0.051183	3.642254
261.889078	4542.595687	7.238886	-0.051248	3.645424
262.186326	4550.605908	7.243891	-0.051309	3.648588
262.489067	4558.663306	7.248896	-0.051371	3.651768
263.116603	4566.649442	7.253901	-0.051493	3.654926
263.365803	4574.644654	7.258906	-0.051544	3.658074
263.709041	4582.719066	7.263910	-0.051613	3.661253
264.357595	4590.643203	7.268915	-0.051739	3.664379
264.224113	4598.788966	7.273920	-0.051720	3.667567
264.687799	4606.836554	7.278925	-0.051811	3.670731
264.467073	4614.856373	7.283930	-0.051775	3.673862
264.679220	4622.913835	7.288934	-0.051820	3.677017
265.003524	4630.881037	7.293939	-0.051885	3.680137
265.784320	4638.755025	7.298944	-0.052036	3.683231
265.662592	4646.948427	7.303949	-0.052019	3.686422
265.866724	4654.938242	7.308954	-0.052062	3.689539
266.545629	4662.970866	7.313958	-0.052193	3.692684
267.061731	4670.960635	7.318963	-0.052295	3.695804
267.229453	4678.971283	7.323968	-0.052331	3.698921
267.607853	4687.051818	7.328973	-0.052407	3.702067
267.985678	4695.012210	7.333978	-0.052482	3.705165
268.058167	4703.098213	7.338982	-0.052501	3.708300
268.386645	4711.160294	7.343987	-0.052567	3.711430
268.715887	4719.191339	7.348992	-0.052634	3.714546
268.992058	4727.205331	7.353997	-0.052690	3.717651
269.425701	4735.168825	7.359002	-0.052776	3.720737
269.698732	4743.166728	7.364006	-0.052832	3.723831
270.140560	4751.217006	7.369011	-0.052920	3.726946
270.296964	4759.249980	7.374016	-0.052954	3.730044
271.021809	4767.241170	7.379021	-0.053094	3.733138
271.264065	4775.296777	7.384026	-0.053145	3.736243
271.304640	4783.324356	7.389030	-0.053157	3.739328
271.728991	4791.337783	7.394035	-0.053242	3.742416
272.022836	4799.332262	7.399040	-0.053301	3.745490
272.492066	4807.367776	7.404045	-0.053394	3.748582
272.568154	4815.450886	7.409050	-0.053413	3.751679
273.007544	4823.441550	7.414054	-0.053500	3.754748
273.080144	4831.450932	7.419059	-0.053519	3.757812
273.560143	4839.426246	7.424064	-0.053614	3.760871
273.802607	4847.482253	7.429069	-0.053664	3.763952
274.093561	4855.494413	7.434074	-0.053723	3.767015
274.706787	4863.497006	7.439078	-0.053843	3.770080
274.287199	4871.626268	7.444083	-0.053770	3.773165
274.744373	4879.633182	7.449088	-0.053860	3.776222
274.941406	4887.630184	7.454093	-0.053902	3.779267
275.213566	4895.615072	7.459098	-0.053958	3.782307
275.537125	4903.630473	7.464102	-0.054023	3.785357
276.209320	4911.634207	7.469107	-0.054154	3.788408
276.359847	4919.737048	7.474112	-0.054187	3.791482
276.808709	4927.693734	7.479117	-0.054276	3.794505
276.971198	4935.732312	7.484122	-0.054311	3.797550
277.082136	4943.783875	7.489126	-0.054337	3.800596
277.437008	4951.737790	7.494131	-0.054408	3.803608
277.723100	4959.806622	7.499136	-0.054467	3.806660
277.907683	4967.850106	7.504141	-0.054506	3.809697
277.939257	4975.867054	7.509146	-0.054517	3.812719
278.315549	4983.921088	7.514150	-0.054593	3.815760
278.730893	4991.873109	7.519155	-0.054675	3.818761
278.787735	4999.916136	7.524160	-0.054691	3.821785
279.101261	5007.953610	7.529165	-0.054754	3.824811
279.619166	5015.944685	7.534170	-0.054856	3.827822
279.838555	5023.999087	7.539174	-0.054902	3.830847
280.345045	5031.988020	7.544179	-0.055001	3.833851
280.802013	5039.986358	7.549184	-0.055092	3.836856
280.902489	5048.070489	7.554189	-0.055116	3.839883
281.042607	5056.063486	7.559194	-0.055147	3.842873
281.230934	5064.137738	7.564198	-0.055187	3.845893
281.422422	5072.177237	7.569203	-0.055228	3.848898
282.054662	5080.136505	7.574208	-0.055351	3.851880
282.467080	5088.176066	7.579213	-0.055433	3.854884
282.745524	5096.184478	7.584218	-0.055490	3.857872
282.900779	5104.239012	7.589222	-0.055524	3.860872
282.852219	5112.291339	7.594227	-0.055520	3.863865
283.379590	5120.257484	7.599232	-0.055624	3.866835
284.265596	5128.259335	7.604237	-0.055794	3.869824
284.425082	5136.370221	7.609242	-0.055829	3.872835
284.605280	5144.498975	7.614246	-0.055867	3.875851
285.220525	5152.336506	7.619251	-0.055987	3.878766
285.835422	5160.348193	7.624256	-0.056107	3.881743
285.868473	5168.354744	7.629261	-0.056118	3.884704
286.200624	5176.377897	7.634266	-0.056185	3.887675
286.440294	5184.438674	7.639270	-0.056235	3.890656
286.691127	5192.446707	7.644275	-0.056287	3.893615
286.584002	5200.524640	7.649280	-0.056272	3.896590
287.136324	5208.450561	7.654285	-0.056380	3.899520
287.480091	5216.448356	7.659290	-0.056449	3.902471
287.526877	5224.550004	7.664294	-0.056463	3.905451
287.937443	5232.512411	7.669299	-0.056545	3.908385
288.269733	5240.563454	7.674304	-0.056612	3.911348
288.507238	5248.576468	7.679309	-0.056661	3.914292
288.974381	5256.564605	7.684314	-0.056753	3.917230
289.339611	5264.620643	7.689318	-0.056827	3.920189
289.605592	5272.596909	7.694323	-0.056881	3.923114
289.501803	5280.679919	7.699328	-0.056867	3.926068
289.942959	5288.689853	7.704333	-0.056955	3.929005
289.974246	5296.743739	7.709338	-0.056966	3.931947
290.261870	5304.809098	7.714342	-0.057024	3.934896
290.514460	5312.808813	7.719347	-0.057077	3.937818
290.797083	5320.790744	7.724352	-0.057134	3.940732
291.220812	5328.772271	7.729357	-0.057218	3.943646
291.300572	5336.809370	7.734362	-0.057239	3.946572
292.073210	5344.791144	7.739366	-0.057388	3.949489
292.209100	5352.899393	7.744371	-0.057418	3.952437
292.530581	5360.857206	7.749376	-0.057483	3.955332
292.857910	5368.925726	7.754381	-0.057549	3.958265
293.133379	5376.960783	7.759386	-0.057606	3.961183
293.599509	5384.871586	7.764390	-0.057698	3.964057
293.780972	5392.990705	7.769395	-0.057737	3.967000
294.096746	5400.962439	7.774400	-0.057801	3.969889
294.642082	5408.983137	7.779405	-0.057907	3.972797
294.193213	5417.094683	7.784410	-0.057829	3.975719
294.493088	5425.095434	7.789414	-0.057890	3.978612
294.869974	5433.129531	7.794419	-0.057965	3.981516
295.192636	5441.011990	7.799424	-0.058031	3.984362
295.846723	5449.106948	7.804429	-0.058158	3.987289
296.379138	5457.069111	7.809434	-0.058262	3.990163
296.400135	5465.166222	7.814438	-0.058271	3.993075
296.708251	5473.185018	7.819443	-0.058334	3.995962
296.765108	5481.193976	7.824448	-0.058349	3.998838
297.227423	5489.236355	7.829453	-0.058441	4.001732
297.431960	5497.148073	7.834458	-0.058484	4.004572
297.258338	5505.287413	7.839462	-0.058457	4.007485
297.381794	5513.310410	7.844467	-0.058485	4.010360
297.599293	5521.343529	7.849472	-0.058531	4.013237
298.060881	5529.369336	7.854477	-0.058622	4.016114
298.270988	5537.321033	7.859482	-0.058666	4.018958
298.569079	5545.374982	7.864486	-0.058727	4.021838
298.956404	5553.323024	7.869491	-0.058804	4.024680
299.462371	5561.364261	7.874496	-0.058903	4.027555
299.684424	5569.420976	7.879501	-0.058950	4.030428
299.910416	5577.497400	7.884506	-0.058997	4.033307
300.202287	5585.546850	7.889510	-0.059057	4.036174
300.872010	5593.426015	7.894515	-0.059187	4.038986
300.825477	5601.497992	7.899520	-0.059183	4.041852
301.368392	5609.439247	7.904525	-0.059289	4.044679
301.705877	5617.487928	7.909530	-0.059358	4.047539
301.810905	5625.529000	7.914534	-0.059382	4.050391
301.741182	5633.632028	7.919539	-0.059375	4.053260
302.251296	5641.641088	7.924544	-0.059475	4.056102
302.789029	5649.610623	7.929549	-0.059580	4.058929
303.229286	5657.570766	7.934554	-0.059667	4.061750
303.551852	5665.593042	7.939558	-0.059732	4.064588
304.005031	5673.641075	7.944563	-0.059822	4.067435
304.205526	5681.681929	7.949568	-0.059864	4.070274
304.229207	5689.767978	7.954573	-0.059874	4.073124
304.442524	5697.768248	7.959578	-0.059919	4.075945
304.958036	5705.732022	7.964582	-0.060020	4.078755
305.111796	5713.802075	7.969587	-0.060054	4.081596
305.273033	5721.771757	7.974592	-0.060089	4.084399
305.805725	5729.804330	7.979597	-0.060194	4.087228
306.246953	5737.778885	7.984602	-0.060281	4.090033
306.501338	5745.864827	7.989606	-0.060333	4.092872
306.787514	5753.916864	7.994611	-0.060392	4.095698
306.984374	5761.918517	7.999616	-0.060434	4.098503
307.709646	5769.929979	8.004621	-0.060574	4.101318
308.184457	5777.852982	8.009626	-0.060668	4.104095
308.436334	5785.944303	8.014630	-0.060720	4.106927
307.999975	5794.074469	8.019635	-0.060644	4.109760
308.630878	5802.019543	8.024640	-0.060766	4.112541
308.977107	5810.039853	8.029645	-0.060836	4.115343
309.202538	5818.022197	8.034650	-0.060883	4.118129
309.309131	5826.080210	8.039654	-0.060908	4.120936
309.786314	5834.043928	8.044659	-0.061002	4.123715
309.810951	5842.118957	8.049664	-0.061012	4.126524
309.957725	5850.119264	8.054669	-0.061044	4.129306
310.305155	5858.133434	8.059674	-0.061114	4.132095
310.962701	5866.071013	8.064678	-0.061242	4.134858
310.972495	5874.165120	8.069683	-0.061249	4.137666
311.335319	5882.167451	8.074688	-0.061322	4.140445
311.518211	5890.200190	8.079693	-0.061361	4.143229
311.761685	5898.184697	8.084698	-0.061411	4.145997
312.020052	5906.255342	8.089702	-0.061465	4.148792
312.359708	5914.305012	8.094707	-0.061533	4.151579
312.447186	5922.210516	8.099712	-0.061555	4.154311
313.130939	5930.243018	8.104717	-0.061687	4.157092
313.218881	5938.255167	8.109722	-0.061709	4.159858
313.492044	5946.290362	8.114726	-0.061765	4.162631
313.629502	5954.332357	8.119731	-0.061796	4.165403
313.737898	5962.398971	8.124736	-0.061821	4.168182
314.670205	5970.375949	8.129741	-0.062000	4.170938
315.006423	5978.359995	8.134746	-0.062067	4.173687
315.055365	5986.466955	8.139750	-0.062082	4.176473
315.502314	5994.408794	8.144755	-0.062170	4.179206
315.698228	6002.485928	8.149760	-0.062212	4.181980
315.981005	6010.468926	8.154765	-0.062270	4.184721
316.410438	6018.474948	8.159770	-0.062355	4.187469
316.710376	6026.540155	8.164774	-0.062416	4.190235
317.319707	6034.562732	8.169779	-0.062535	4.192987
317.243408	6042.643582	8.174784	-0.062526	4.195750
317.578485	6050.631633	8.179789	-0.062593	4.198484
317.716464	6058.599716	8.184794	-0.062624	4.201207
318.387463	6066.563296	8.189798	-0.062754	4.203933
318.446707	6074.691091	8.194803	-0.062770	4.206706
318.449209	6082.653008	8.199808	-0.062776	4.209420
319.513285	6090.594985	8.204813	-0.062979	4.212137
319.500941	6098.666977	8.209818	-0.062982	4.214885
319.797633	6106.731367	8.214822	-0.063043	4.217631
319.743065	6114.785934	8.219827	-0.063038	4.220369
320.156338	6122.700974	8.224832	-0.063120	4.223063
320.227927	6130.782158	8.229837	-0.063138	4.225807
320.667908	6138.753774	8.234842	-0.063225	4.228517
320.948352	6146.841674	8.239846	-0.063283	4.231262
321.297527	6154.813893	8.244851	-0.063353	4.233968
321.603848	6162.851726	8.249856	-0.063415	4.236693
321.957853	6170.836167	8.254861	-0.063486	4.239399
321.958157	6178.909768	8.259866	-0.063492	4.242129
322.731334	6186.827110	8.264870	-0.063641	4.244813
322.622177	6194.946901	8.269875	-0.063626	4.247555
322.767687	6202.918904	8.274880	-0.063658	4.250247
323.067949	6210.988564	8.279885	-0.063719	4.252972
323.119481	6219.029305	8.284890	-0.063734	4.255683
323.758474	6226.923279	8.289894	-0.063858	4.258349
324.273074	6234.990333	8.294899	-0.063959	4.261070
324.817163	6242.925451	8.299904	-0.064065	4.263746
325.122829	6251.015781	8.304909	-0.064127	4.266469
325.285662	6259.038418	8.309914	-0.064163	4.269166
325.341222	6267.155784	8.314918	-0.064179	4.271893
325.713749	6275.065496	8.319923	-0.064253	4.274551
325.505671	6283.176512	8.324928	-0.064220	4.277269
325.655682	6291.165098	8.329933	-0.064253	4.279948
326.015688	6299.164056	8.334938	-0.064325	4.282631
326.751723	6307.071881	8.339942	-0.064467	4.285285
326.713634	6315.164088	8.344947	-0.064465	4.287992
326.865174	6323.239379	8.349952	-0.064499	4.290693
328.010481	6331.176835	8.354957	-0.064717	4.293355
328.142505	6339.214456	8.359962	-0.064747	4.296040
328.518758	6347.234695	8.364966	-0.064822	4.298720
328.910976	6355.237197	8.369971	-0.064900	4.301392
329.156927	6363.210294	8.374976	-0.064951	4.304051
329.818874	6371.267514	8.379981	-0.065080	4.306741
330.249029	6379.291996	8.384986	-0.065165	4.309415
329.806733	6387.396804	8.389990	-0.065088	4.312107
330.445725	6395.335931	8.394995	-0.065212	4.314752
331.180099	6403.284343	8.400000	-0.065354	4.317399
331.139434	6411.371361	8.405005	-0.065351	4.320083
331.364003	6419.315560	8.410010	-0.065398	4.322721
331.825007	6427.358651	8.415014	-0.065489	4.325392
331.905923	6435.424781	8.420019	-0.065510	4.328066
331.815047	6443.501095	8.425024	-0.065498	4.330740
332.180517	6451.480691	8.430029	-0.065571	4.333384
332.467060	6459.510650	8.435034	-0.065630	4.336042
332.822895	6467.443861	8.440038	-0.065701	4.338667
333.109731	6475.532079	8.445043	-0.065760	4.341342
333.617541	6483.428190	8.450048	-0.065859	4.343953
333.475313	6491.602825	8.455053	-0.065838	4.346649
333.860345	6499.540144	8.460058	-0.065915	4.349269
334.604830	6507.601148	8.465062	-0.066059	4.351931
334.761386	6515.598277	8.470067	-0.066093	4.354566
335.011926	6523.584918	8.475072	-0.066145	4.357197
335.089839	6531.633520	8.480077	-0.066165	4.359845
335.270475	6539.629678	8.485082	-0.066204	4.362475
335.264991	6547.650041	8.490086	-0.066208	4.365110
335.208486	6555.682073	8.495091	-0.066202	4.367747
335.759251	6563.693464	8.500096	-0.066310	4.370380
335.980712	6571.732195	8.505101	-0.066357	4.373017
336.459565	6579.698003	8.510106	-0.066451	4.375631
336.761876	6587.728736	8.515110	-0.066512	4.378264
337.523780	6595.708124	8.520115	-0.066659	4.380881
337.516909	6603.720848	8.525120	-0.066663	4.383502
337.276167	6611.852994	8.530125	-0.066624	4.386159
338.040631	6619.782331	8.535130	-0.066771	4.388755
338.421201	6627.826691	8.540134	-0.066847	4.391385
338.346050	6635.893679	8.545139	-0.066839	4.394017
338.446114	6643.945764	8.550144	-0.066862	4.396644
338.919187	6651.886244	8.555149	-0.066956	4.399235
338.834875	6659.973660	8.560154	-0.066945	4.401869
339.091391	6667.951971	8.565159	-0.066998	4.404468
339.519448	6675.976982	8.570163	-0.067083	4.407082
339.654312	6683.973989	8.575168	-0.067113	4.409683
339.802544	6692.051448	8.580173	-0.067146	4.412309
340.407087	6699.967764	8.585178	-0.067264	4.414884
340.635322	6708.062192	8.590183	-0.067311	4.417512
340.691646	6716.088559	8.595187	-0.067327	4.420116
340.722403	6724.106656	8.600192	-0.067338	4.422716
341.421929	6732.123587	8.605197	-0.067473	4.425318
341.567550	6740.168596	8.610202	-0.067506	4.427924
341.984172	6748.189656	8.615207	-0.067589	4.430522
342.348804	6756.206822	8.620211	-0.067662	4.433117
342.360208	6764.215412	8.625216	-0.067669	4.435706
342.773018	6772.232705	8.630221	-0.067751	4.438298
342.847594	6780.291323	8.635226	-0.067770	4.440900
343.144709	6788.257241	8.640231	-0.067831	4.443472
343.688469	6796.241407	8.645235	-0.067937	4.446049
343.703055	6804.246498	8.650240	-0.067945	4.448629
344.341465	6812.344494	8.655245	-0.068069	4.451241
344.641112	6820.335314	8.660250	-0.068130	4.453815
345.029365	6828.370313	8.665255	-0.068207	4.456402
345.532374	6836.343355	8.670259	-0.068306	4.458968
345.404547	6844.400463	8.675264	-0.068288	4.461556
345.675683	6852.378615	8.680269	-0.068343	4.464120
345.695287	6860.469184	8.685274	-0.068352	4.466716
345.871018	6868.474649	8.690279	-0.068390	4.469285
346.053406	6876.531461	8.695283	-0.068429	4.471869
346.492495	6884.451079	8.700288	-0.068516	4.474408
346.963391	6892.504653	8.705293	-0.068609	4.476989
347.627159	6900.371184	8.710298	-0.068738	4.479510
347.538547	6908.504228	8.715303	-0.068726	4.482111
348.153183	6916.448203	8.720307	-0.068846	4.484653
348.350697	6924.540095	8.725312	-0.068888	4.487239
348.378927	6932.584098	8.730317	-0.068899	4.489807
348.666852	6940.593300	8.735322	-0.068957	4.492364
349.347076	6948.526028	8.740327	-0.069089	4.494897
349.364709	6956.603721	8.745331	-0.069098	4.497471
349.803070	6964.648745	8.750336	-0.069184	4.500036
350.403931	6972.628972	8.755341	-0.069301	4.502579
350.322637	6980.647253	8.760346	-0.069292	4.505130
350.754746	6988.681977	8.765351	-0.069377	4.507686
351.195471	6996.687939	8.770355	-0.069464	4.510232
351.373011	7004.700469	8.775360	-0.069503	4.512778
351.844256	7012.691857	8.780365	-0.069596	4.515316
351.768278	7020.755651	8.785370	-0.069587	4.517874
351.992491	7028.786453	8.790375	-0.069634	4.520422
352.049358	7036.762465	8.795379	-0.069649	4.522950
352.297321	7044.714467	8.800384	-0.069701	4.525469
353.019585	7052.762124	8.805389	-0.069840	4.528019
352.550260	7060.819947	8.810394	-0.069758	4.530567
353.298690	7068.734565	8.815399	-0.069903	4.533071
353.698686	7076.857625	8.820403	-0.069982	4.535640
353.561696	7084.837942	8.825408	-0.069962	4.538160
353.746098	7092.873287	8.830413	-0.070002	4.540697
354.100601	7100.850393	8.835418	-0.070073	4.543214
354.086015	7108.911389	8.840423	-0.070075	4.545756
354.368956	7116.929899	8.845427	-0.070133	4.548283
354.489437	7124.972118	8.850432	-0.070161	4.550817
354.901389	7132.979925	8.855437	-0.070243	4.553338
355.243936	7140.922381	8.860442	-0.070312	4.555838
355.545111	7148.903412	8.865447	-0.070373	4.558348
356.053884	7156.966002	8.870451	-0.070473	4.560883
356.651721	7164.889487	8.875456	-0.070589	4.563372
356.492368	7173.046473	8.880461	-0.070565	4.565932
356.468358	7181.015974	8.885466	-0.070565	4.568433
356.919528	7189.106355	8.890471	-0.070655	4.570970
356.987932	7197.087165	8.895475	-0.070673	4.573471
357.089287	7205.122037	8.900480	-0.070697	4.575988
357.556204	7213.092441	8.905485	-0.070789	4.578484
357.551828	7221.110921	8.910490	-0.070793	4.580992
357.916822	7229.091878	8.915495	-0.070866	4.583488
358.336832	7237.177985	8.920499	-0.070950	4.586016
358.702968	7245.147008	8.925504	-0.071023	4.588505
358.836934	7253.213654	8.930509	-0.071053	4.591023
358.807578	7261.198448	8.935514	-0.071053	4.593514
359.456192	7269.217664	8.940519	-0.071179	4.596016
359.768014	7277.195816	8.945523	-0.071242	4.598502
359.812259	7285.237633	8.950528	-0.071255	4.601007
360.046824	7293.245017	8.955533	-0.071304	4.603500
360.486883	7301.254098	8.960538	-0.071391	4.605992
360.639103	7309.247581	8.965543	-0.071425	4.608478
360.751692	7317.328975	8.970547	-0.071451	4.610990
361.125649	7325.264242	8.975552	-0.071526	4.613455
361.297817	7333.374475	8.980557	-0.071563	4.615973
361.608873	7341.316739	8.985562	-0.071626	4.618437
361.888110	7349.405445	8.990567	-0.071683	4.620946
362.154955	7357.344528	8.995571	-0.071738	4.623407
362.388528	7365.395890	9.000576	-0.071787	4.625901
362.991891	7373.409669	9.005581	-0.071905	4.628382
363.357463	7381.420304	9.010586	-0.071978	4.630861
363.460176	7389.486246	9.015591	-0.072002	4.633356
363.640778	7397.559519	9.020595	-0.072041	4.635851
364.367624	7405.398085	9.025600	-0.072181	4.638273
364.852856	7413.457686	9.030605	-0.072277	4.640761
364.815437	7421.507979	9.035610	-0.072275	4.643245
365.496707	7429.448852	9.040615	-0.072407	4.645695
365.405928	7437.579775	9.045619	-0.072396	4.648201
365.691633	7445.512313	9.050624	-0.072454	4.650645
366.024398	7453.576934	9.055629	-0.072521	4.653128
366.191637	7461.575930	9.060634	-0.072557	4.655590
366.706815	7469.560127	9.065639	-0.072658	4.658046
366.909679	7477.605404	9.070643	-0.072701	4.660519
366.950007	7485.650826	9.075648	-0.072714	4.662991
367.258030	7493.659147	9.080653	-0.072777	4.665450
368.062282	7501.627708	9.085658	-0.072932	4.667895
368.289044	7509.686425	9.090663	-0.072979	4.670367
368.737708	7517.751924	9.095667	-0.073068	4.672840
369.106188	7525.740199	9.100672	-0.073142	4.675288
369.336324	7533.763108	9.105677	-0.073190	4.677745
369.524501	7541.722904	9.110682	-0.073230	4.680181
369.764922	7549.711556	9.115687	-0.073280	4.682625
370.237058	7557.732680	9.120691	-0.073373	4.685077
370.495694	7565.756560	9.125696	-0.073426	4.687529
370.465488	7573.804306	9.130701	-0.073426	4.689988
370.535447	7581.819775	9.135706	-0.073444	4.692435
370.906540	7589.809806	9.140711	-0.073518	4.694872
371.039559	7597.885184	9.145715	-0.073548	4.697335
370.968640	7605.836010	9.150720	-0.073540	4.699759
371.391079	7613.879025	9.155725	-0.073624	4.702208
371.278885	7621.915927	9.160730	-0.073608	4.704656
371.481575	7629.958379	9.165735	-0.073651	4.707103
371.853516	7637.960717	9.170739	-0.073726	4.709537
371.895479	7646.018135	9.175744	-0.073739	4.711986
372.248016	7653.980617	9.180749	-0.073809	4.714405
372.687850	7661.971439	9.185754	-0.073897	4.716831
373.222001	7669.916653	9.190759	-0.074001	4.719242
373.785062	7677.963066	9.195763	-0.074111	4.721682
373.642791	7685.925312	9.200768	-0.074090	4.724097
373.640111	7694.095415	9.205773	-0.074095	4.726573
373.970246	7702.028570	9.210778	-0.074161	4.728975
374.335187	7710.114652	9.215783	-0.074234	4.731423
374.570000	7718.088624	9.220787	-0.074283	4.733835
375.024749	7726.114722	9.225792	-0.074373	4.736261
375.316179	7734.125382	9.230797	-0.074433	4.738682
375.290175	7742.155547	9.235802	-0.074433	4.741108
375.721802	7750.095991	9.240807	-0.074518	4.743505
376.321779	7758.126748	9.245811	-0.074635	4.745927
376.078391	7766.228790	9.250816	-0.074595	4.748372
376.006600	7774.323860	9.255821	-0.074587	4.750813
376.340421	7782.274049	9.260826	-0.074654	4.753208
376.959708	7790.274319	9.265831	-0.074775	4.755616
376.907079	7798.299073	9.270835	-0.074770	4.758031
377.597645	7806.203622	9.275840	-0.074904	4.760408
378.055649	7814.257773	9.280845	-0.074995	4.762829
378.073499	7822.281009	9.285850	-0.075003	4.765240
378.350082	7830.334651	9.290855	-0.075060	4.767659
378.475241	7838.365052	9.295859	-0.075088	4.770070
378.754155	7846.343836	9.300864	-0.075145	4.772463
379.078478	7854.373001	9.305869	-0.075211	4.774871
379.126220	7862.396258	9.310874	-0.075225	4.777276
379.436015	7870.384602	9.315879	-0.075288	4.779668
379.528880	7878.494706	9.320883	-0.075310	4.782097
379.115728	7886.461677	9.325888	-0.075239	4.784483
379.943828	7894.458535	9.330893	-0.075398	4.786873
380.002783	7902.526367	9.335898	-0.075414	4.789286
380.235940	7910.546979	9.340903	-0.075463	4.791682
380.555323	7918.513110	9.345907	-0.075527	4.794061
380.635599	7926.567341	9.350912	-0.075548	4.796465
380.938011	7934.546672	9.355917	-0.075609	4.798845
381.322451	7942.570863	9.360922	-0.075686	4.801237
381.461141	7950.522873	9.365927	-0.075717	4.803608
381.538765	7958.578715	9.370931	-0.075736	4.806008
382.024818	7966.508537	9.375936	-0.075832	4.808368
381.822683	7974.710543	9.380941	-0.075800	4.810810
382.035279	7982.625036	9.385946	-0.075844	4.813164
381.959922	7990.047198	9.390951	-0.075835	4.815372
382.255203	7994.637326	9.395955	-0.075893	4.816735

382.458828	7997.210462	9.400960	-0.075933	4.817499
382.403134	7998.453575	9.405965	-0.075923	4.817869
382.786023	7998.859007	9.410970	-0.075995	4.817988
383.302038	7999.740112	9.415975	-0.076091	4.818247
383.172834	7999.777244	9.420979	-0.076067	4.818259
383.305336	7999.766418	9.425984	-0.076092	4.818255
384.035286	7999.772055	9.430989	-0.076228	4.818254
383.794861	7999.759353	9.435994	-0.076183	4.818251
383.758339	7999.813495	9.440999	-0.076176	4.818267
384.039977	7999.798377	9.446003	-0.076228	4.818262
384.225748	7999.770409	9.451008	-0.076263	4.818253
384.698455	7999.746310	9.456013	-0.076351	4.818244
384.247551	7999.786458	9.461018	-0.076267	4.818257
384.553804	7999.789535	9.466023	-0.076324	4.818257
384.540559	7999.817724	9.471027	-0.076321	4.818265
384.367350	7999.770203	9.476032	-0.076289	4.818252
384.805079	7999.837048	9.481037	-0.076371	4.818270
384.714736	7999.804303	9.486042	-0.076354	4.818261
384.943475	7999.805285	9.491047	-0.076396	4.818260
385.139927	7999.839456	9.496051	-0.076433	4.818270
385.623842	7999.801851	9.501056	-0.076523	4.818256
385.742868	7999.793998	9.506061	-0.076545	4.818254
385.799261	7999.739066	9.511066	-0.076555	4.818237
385.803898	7999.785359	9.516071	-0.076556	4.818251
385.882422	7999.754893	9.521075	-0.076571	4.818241
385.797716	7999.750595	9.526080	-0.076555	4.818241
385.839665	7999.780579	9.531085	-0.076563	4.818249
386.040497	7999.775932	9.536090	-0.076600	4.818247
385.917624	7999.793184	9.541095	-0.076577	4.818253
386.238384	7999.768090	9.546099	-0.076637	4.818244
386.262404	7999.875591	9.551104	-0.076641	4.818276
386.492767	7999.801991	9.556109	-0.076684	4.818253
386.311961	7999.888864	9.561114	-0.076651	4.818280
386.571995	7999.826173	9.566119	-0.076699	4.818260
386.493992	7999.882910	9.571123	-0.076684	4.818277
386.597568	7999.858036	9.576128	-0.076704	4.818269
386.975036	7999.866284	9.581133	-0.076774	4.818270
386.480950	7999.931062	9.586138	-0.076682	4.818291
386.482808	7999.828106	9.591143	-0.076682	4.818261
386.788320	7999.878464	9.596147	-0.076739	4.818275
386.829217	7999.864303	9.601152	-0.076747	4.818270
387.222692	7999.805516	9.606157	-0.076820	4.818251
386.805648	7999.879741	9.611162	-0.076742	4.818275
386.835705	7999.886448	9.616167	-0.076748	4.818277
386.995859	7999.804545	9.621171	-0.076777	4.818252
387.084160	7999.862478	9.626176	-0.076794	4.818269
386.858379	7999.849968	9.631181	-0.076752	4.818266
386.631631	7999.814328	9.636186	-0.076709	4.818256
386.638431	7999.901633	9.641191	-0.076711	4.818282
386.879675	7999.862856	9.646195	-0.076756	4.818270
386.876802	7999.801868	9.651200	-0.076755	4.818251
387.037930	7999.853429	9.656205	-0.076785	4.818266
387.065785	7999.838041	9.661210	-0.076790	4.818261
387.395210	7999.822523	9.666215	-0.076851	4.818256
387.246900	7999.846786	9.671219	-0.076824	4.818263
387.796328	7999.946679	9.676224	-0.076926	4.818291
387.678591	7999.806377	9.681229	-0.076904	4.818250
387.549623	7999.836156	9.686234	-0.076880	4.818259
387.182224	7999.873222	9.691239	-0.076812	4.818271
387.095272	7999.859435	9.696243	-0.076795	4.818268
387.003478	7999.837176	9.701248	-0.076778	4.818261
387.376666	7999.870586	9.706253	-0.076848	4.818270
387.760698	7999.867366	9.711258	-0.076919	4.818267
387.703754	7999.805646	9.716263	-0.076908	4.818249
387.271373	7999.868104	9.721267	-0.076828	4.818270
387.060015	7999.844230	9.726272	-0.076789	4.818263
387.178504	7999.869996	9.731277	-0.076811	4.818270
387.667711	7999.952262	9.736282	-0.076902	4.818293
387.671089	7999.849324	9.741287	-0.076902	4.818262
387.652487	7999.858527	9.746291	-0.076899	4.818265
387.451785	7999.844254	9.751296	-0.076861	4.818262
387.520118	7999.880902	9.756301	-0.076874	4.818272
387.448784	7999.873630	9.761306	-0.076861	4.818270
387.692340	7999.870613	9.766311	-0.076906	4.818269
387.679546	7999.874641	9.771315	-0.076904	4.818270
387.914606	7999.806358	9.776320	-0.076947	4.818249
387.575476	7999.947837	9.781325	-0.076884	4.818292
388.329067	7999.785683	9.786330	-0.077024	4.818241
388.189388	7999.874164	9.791335	-0.076998	4.818268
387.879352	7999.832141	9.796339	-0.076941	4.818256
387.461485	7999.849610	9.801344	-0.076863	4.818263
387.870448	7999.834116	9.806349	-0.076939	4.818257
387.807814	7999.803844	9.811354	-0.076927	4.818248
388.028172	7999.894038	9.816359	-0.076968	4.818274
387.694760	7999.906342	9.821363	-0.076906	4.818279
387.769373	7999.870569	9.826368	-0.076920	4.818268
388.062964	7999.853517	9.831373	-0.076974	4.818262
388.137390	7999.833503	9.836378	-0.076988	4.818256
388.078701	7999.866334	9.841383	-0.076977	4.818266
388.078121	7999.906254	9.846387	-0.076977	4.818278
387.873359	7999.854095	9.851392	-0.076939	4.818263
388.518095	7999.827078	9.856397	-0.077059	4.818252
388.757552	7999.887058	9.861402	-0.077104	4.818269
388.840566	7999.913398	9.866407	-0.077119	4.818277
388.794481	7999.803483	9.871411	-0.077110	4.818244
389.204349	7999.970854	9.876416	-0.077187	4.818292
388.738281	7999.830040	9.881421	-0.077100	4.818252
388.704898	7999.795959	9.886426	-0.077093	4.818242
388.968239	7999.903550	9.891431	-0.077143	4.818273
388.568727	7999.841400	9.896435	-0.077068	4.818256
388.815671	7999.970838	9.901440	-0.077114	4.818294
388.751360	7999.813389	9.906445	-0.077102	4.818247
388.805523	7999.893982	9.911450	-0.077112	4.818271
388.620115	7999.813710	9.916455	-0.077077	4.818248
388.994087	7999.810356	9.921459	-0.077147	4.818246
388.823498	7999.890013	9.926464	-0.077115	4.818270
389.111531	7999.866583	9.931469	-0.077169	4.818262
388.965814	7999.808914	9.936474	-0.077142	4.818245
389.131049	7999.832163	9.941479	-0.077172	4.818251
388.761475	7999.914383	9.946483	-0.077104	4.818277
388.843804	7999.821968	9.951488	-0.077119	4.818250
389.086737	7999.854674	9.956493	-0.077164	4.818258
389.360273	7999.856268	9.961498	-0.077215	4.818258
389.364179	7999.939336	9.966503	-0.077216	4.818282
389.408626	7999.816983	9.971507	-0.077224	4.818246
389.335173	7999.861174	9.976512	-0.077210	4.818259
389.361565	7999.830002	9.981517	-0.077215	4.818250
389.441690	7999.798506	9.986522	-0.077230	4.818240
389.363221	7999.823714	9.991527	-0.077215	4.818248
389.436815	7999.906673	9.996531	-0.077229	4.818272
389.378759	7999.885919	10.001536	-0.077218	4.818266
389.571868	7999.842289	10.006541	-0.077254	4.818253
389.823341	7999.882468	10.011546	-0.077301	4.818264
389.507313	7999.830902	10.016551	-0.077242	4.818250
389.260108	7999.951558	10.021555	-0.077196	4.818286
389.249767	7999.801142	10.026560	-0.077194	4.818242
389.546800	7999.886072	10.031565	-0.077249	4.818266
389.644476	7999.780202	10.036570	-0.077267	4.818234
389.345018	7999.882287	10.041575	-0.077211	4.818265
389.016786	7999.836862	10.046579	-0.077150	4.818253
389.167429	7999.792658	10.051584	-0.077178	4.818240
389.773382	7999.895428	10.056589	-0.077291	4.818268
389.286284	7999.909854	10.061594	-0.077200	4.818274
388.833650	7999.815459	10.066599	-0.077116	4.818248
389.455544	7999.817560	10.071603	-0.077232	4.818246
389.442960	7999.888845	10.076608	-0.077229	4.818267
389.504189	7999.777228	10.081613	-0.077241	4.818234
389.689580	7999.917396	10.086618	-0.077275	4.818275
389.428482	7999.838199	10.091623	-0.077227	4.818252
389.516060	7999.840432	10.096627	-0.077243	4.818252
389.238429	7999.836674	10.101632	-0.077191	4.818252
389.435346	7999.835131	10.106637	-0.077228	4.818251
389.562068	7999.851554	10.111642	-0.077251	4.818256
389.741195	7999.880245	10.116647	-0.077285	4.818263
389.816166	7999.899121	10.121651	-0.077299	4.818269
389.636949	7999.891440	10.126656	-0.077265	4.818267
389.387825	7999.849186	10.131661	-0.077219	4.818256
389.030972	7999.874832	10.136666	-0.077152	4.818265
389.568022	7999.835854	10.141671	-0.077252	4.818251
389.392472	7999.873410	10.146675	-0.077219	4.818263
389.267634	7999.838091	10.151680	-0.077196	4.818253
389.671679	7999.872977	10.156685	-0.077271	4.818261
389.445473	7999.869914	10.161690	-0.077229	4.818261
389.555807	7999.845132	10.166695	-0.077250	4.818254
389.685176	7999.831116	10.171699	-0.077274	4.818249
389.569720	7999.840060	10.176704	-0.077252	4.818252
390.297176	7999.944477	10.181709	-0.077388	4.818280
389.833762	7999.808947	10.186714	-0.077301	4.818242
389.541512	7999.864890	10.191719	-0.077247	4.818260
389.403754	7999.853567	10.196723	-0.077221	4.818257
389.588822	7999.913865	10.201728	-0.077256	4.818274
389.932940	7999.839701	10.206733	-0.077320	4.818251
389.917035	7999.826872	10.211738	-0.077317	4.818247
389.777682	7999.926919	10.216743	-0.077291	4.818277
389.366715	7999.866713	10.221747	-0.077214	4.818261
389.728390	7999.873703	10.226752	-0.077281	4.818261
389.965979	7999.861151	10.231757	-0.077326	4.818257
389.534307	7999.885784	10.236762	-0.077245	4.818266
389.843803	7999.853187	10.241767	-0.077303	4.818255
389.862958	7999.860799	10.246771	-0.077306	4.818257
389.664894	7999.841304	10.251776	-0.077269	4.818252
390.006675	7999.865890	10.256781	-0.077333	4.818258
390.327029	7999.926970	10.261786	-0.077393	4.818275
389.642444	7999.912450	10.266791	-0.077265	4.818273
389.780350	7999.899601	10.271795	-0.077291	4.818269
390.013344	7999.830239	10.276800	-0.077334	4.818247
390.305792	7999.847854	10.281805	-0.077388	4.818251
389.995132	7999.826834	10.286810	-0.077331	4.818246
389.664857	7999.908536	10.291815	-0.077269	4.818272
389.774706	7999.902662	10.296819	-0.077289	4.818270
389.652094	7999.845305	10.301824	-0.077267	4.818253
389.276326	7999.923238	10.306829	-0.077197	4.818278
389.712246	7999.855570	10.311834	-0.077278	4.818256
389.827480	7999.890754	10.316839	-0.077299	4.818266
389.503472	7999.888470	10.321843	-0.077239	4.818267
389.695536	7999.836420	10.326848	-0.077274	4.818251
390.180417	7999.934403	10.331853	-0.077365	4.818278
389.949850	7999.852465	10.336858	-0.077322	4.818254
389.942942	7999.843961	10.341863	-0.077320	4.818252
390.425478	7999.833672	10.346867	-0.077410	4.818247
390.167814	7999.918458	10.351872	-0.077362	4.818273
390.347243	7999.853626	10.356877	-0.077396	4.818253
390.162240	7999.852171	10.361882	-0.077361	4.818253
389.776757	7999.869022	10.366887	-0.077289	4.818260
389.591370	7999.894885	10.371891	-0.077255	4.818268
389.664349	7999.884309	10.376896	-0.077268	4.818265
390.003683	7999.912016	10.381901	-0.077331	4.818272
390.023172	7999.869191	10.386906	-0.077335	4.818259
389.990570	7999.874001	10.391911	-0.077329	4.818261
390.055654	7999.910609	10.396915	-0.077341	4.818271
389.847475	7999.906738	10.401920	-0.077302	4.818271
390.013453	7999.897421	10.406925	-0.077333	4.818267
390.290651	7999.863337	10.411930	-0.077385	4.818256
390.556713	7999.852222	10.416935	-0.077434	4.818252
390.263581	7999.860863	10.421939	-0.077379	4.818256
390.204958	7999.867423	10.426944	-0.077369	4.818258
390.221449	7999.872898	10.431949	-0.077372	4.818259
390.304792	7999.835140	10.436954	-0.077387	4.818248
390.228090	7999.931831	10.441959	-0.077373	4.818277
390.414849	7999.838725	10.446963	-0.077407	4.818248
390.439879	7999.829603	10.451968	-0.077412	4.818246
390.258814	7999.885999	10.456973	-0.077378	4.818263
390.755450	7999.926346	10.461978	-0.077471	4.818273
390.303931	7999.872943	10.466983	-0.077387	4.818259
390.372889	7999.843397	10.471987	-0.077399	4.818250
390.759426	7999.880151	10.476992	-0.077471	4.818259
391.033855	7999.791383	10.481997	-0.077522	4.818232
390.500232	7999.939692	10.487002	-0.077423	4.818278
390.547398	7999.856255	10.492007	-0.077432	4.818253
390.677799	7999.884289	10.497011	-0.077456	4.818261
390.279561	7999.847371	10.502016	-0.077382	4.818251
390.201816	7999.883097	10.507021	-0.077367	4.818262
390.427182	7999.867228	10.512026	-0.077409	4.818257
390.528487	7999.862290	10.517031	-0.077428	4.818255
390.531591	7999.860228	10.522035	-0.077429	4.818254
389.888403	7999.881998	10.527040	-0.077309	4.818263
390.357443	7999.850509	10.532045	-0.077396	4.818252
389.987984	7999.862322	10.537050	-0.077327	4.818257
390.201590	7999.935618	10.542055	-0.077367	4.818278
390.318939	7999.867845	10.547059	-0.077389	4.818257
390.300828	7999.833968	10.552064	-0.077385	4.818247
390.335066	7999.836531	10.557069	-0.077392	4.818248
390.421307	7999.883934	10.562074	-0.077408	4.818262
390.339394	7999.882822	10.567079	-0.077392	4.818262
390.524746	7999.869564	10.572083	-0.077427	4.818257
390.454495	7999.867560	10.577088	-0.077414	4.818257
390.415625	7999.889099	10.582093	-0.077407	4.818263
390.316745	7999.907725	10.587098	-0.077388	4.818269
390.125441	7999.917745	10.592103	-0.077352	4.818273
390.201426	7999.931381	10.597107	-0.077367	4.818277
390.099530	7999.898472	10.602112	-0.077348	4.818267
390.192404	7999.899726	10.607117	-0.077365	4.818267
389.834074	7999.905384	10.612122	-0.077298	4.818270
390.018941	7999.896323	10.617127	-0.077332	4.818267
390.177340	7999.948905	10.622131	-0.077362	4.818282
389.818574	7999.914624	10.627136	-0.077295	4.818273
390.249090	7999.954074	10.632141	-0.077375	4.818283
390.401654	7999.937219	10.637146	-0.077404	4.818278
390.137238	7999.937842	10.642151	-0.077354	4.818279
390.028880	7999.992070	10.647155	-0.077334	4.818295
390.109482	7999.929054	10.652160	-0.077349	4.818276
390.122701	7999.978621	10.657165	-0.077351	4.818291
390.083042	7999.941301	10.662170	-0.077344	4.818280
390.196372	7999.943882	10.667175	-0.077365	4.818280
390.354991	7999.911346	10.672179	-0.077395	4.818270
390.299457	7999.881167	10.677184	-0.077384	4.818261
390.492029	7999.878515	10.682189	-0.077420	4.818260
390.238375	7999.932879	10.687194	-0.077373	4.818277
390.424946	7999.900721	10.692199	-0.077407	4.818267
390.368666	7999.918873	10.697203	-0.077397	4.818272
390.314742	7999.907632	10.702208	-0.077387	4.818269
390.376631	7999.891652	10.707213	-0.077398	4.818264
390.687616	7999.920028	10.712218	-0.077456	4.818271
391.191225	7999.899518	10.717223	-0.077550	4.818263
391.328446	7999.827809	10.722227	-0.077575	4.818241
391.078329	7999.822319	10.727232	-0.077529	4.818241
391.097314	7999.848845	10.732237	-0.077532	4.818249
391.108303	7999.854246	10.737242	-0.077534	4.818250
390.608000	7999.966223	10.742247	-0.077441	4.818285
390.859783	7999.865589	10.747251	-0.077488	4.818255
391.326699	7999.812004	10.752256	-0.077575	4.818237
391.308589	7999.845385	10.757261	-0.077571	4.818247
391.156208	7999.827556	10.762266	-0.077543	4.818242
390.804374	7999.871133	10.767271	-0.077477	4.818256
391.013242	7999.883415	10.772275	-0.077516	4.818259
390.822389	7999.861913	10.777280	-0.077481	4.818254
391.106134	7999.851038	10.782285	-0.077533	4.818249
390.695683	7999.898025	10.787290	-0.077457	4.818265
390.711129	7999.954979	10.792295	-0.077460	4.818282
391.063740	7999.842048	10.797299	-0.077525	4.818247
390.967595	7999.850202	10.802304	-0.077508	4.818250
390.776238	7999.905409	10.807309	-0.077472	4.818267
390.897773	7999.876574	10.812314	-0.077494	4.818258
391.187502	7999.862628	10.817319	-0.077548	4.818252
390.966132	7999.884850	10.822323	-0.077507	4.818260
390.954009	7999.846851	10.827328	-0.077505	4.818249
391.442458	7999.838746	10.832333	-0.077596	4.818244
391.224011	7999.856805	10.837338	-0.077555	4.818251
391.056912	7999.852438	10.842343	-0.077524	4.818250
390.967903	7999.902725	10.847347	-0.077507	4.818265
391.040234	7999.957297	10.852352	-0.077521	4.818281
390.789093	7999.907655	10.857357	-0.077474	4.818267
390.550781	7999.882358	10.862362	-0.077429	4.818261
390.707164	7999.882370	10.867367	-0.077459	4.818260
390.891032	7999.889059	10.872371	-0.077493	4.818261
390.791546	7999.848827	10.877376	-0.077474	4.818250
391.202267	7999.884859	10.882381	-0.077551	4.818259
391.076980	7999.888414	10.887386	-0.077527	4.818261
390.830946	7999.891387	10.892391	-0.077481	4.818262
390.755949	7999.950270	10.897395	-0.077467	4.818280
390.730075	7999.896321	10.902400	-0.077463	4.818264
391.232420	7999.877896	10.907405	-0.077556	4.818257
391.292882	7999.842981	10.912410	-0.077567	4.818246
391.159279	7999.864289	10.917415	-0.077542	4.818253
391.132279	7999.922772	10.922419	-0.077537	4.818270
391.060820	7999.883969	10.927424	-0.077524	4.818259
390.955151	7999.903554	10.932429	-0.077504	4.818265
391.198610	7999.905795	10.937434	-0.077549	4.818265
390.939698	7999.912797	10.942439	-0.077501	4.818268
391.258684	7999.930774	10.947443	-0.077561	4.818272
390.967741	7999.942596	10.952448	-0.077506	4.818277
391.165511	7999.922150	10.957453	-0.077543	4.818270
391.466932	7999.868428	10.962458	-0.077599	4.818253
391.494287	7999.861439	10.967463	-0.077604	4.818251
391.583177	7999.893116	10.972467	-0.077621	4.818260
391.506863	7999.834279	10.977472	-0.077607	4.818243
391.495532	7999.891923	10.982477	-0.077604	4.818260
391.757801	7999.856587	10.987482	-0.077653	4.818248
391.679548	7999.850270	10.992487	-0.077639	4.818247
391.464962	7999.910417	10.997491	-0.077599	4.818265
390.927410	7999.908392	11.002496	-0.077498	4.818267
391.201262	7999.932063	11.007501	-0.077549	4.818273
391.440117	7999.864883	11.012506	-0.077594	4.818252
391.548650	7999.875808	11.017511	-0.077614	4.818255
391.548102	7999.951463	11.022515	-0.077614	4.818277
391.315476	7999.986144	11.027520	-0.077571	4.818289
391.311581	7999.917779	11.032525	-0.077570	4.818268
391.230991	7999.890412	11.037530	-0.077555	4.818261
391.304272	7999.868281	11.042535	-0.077568	4.818254
391.657934	7999.874117	11.047539	-0.077634	4.818254
391.312442	7999.894659	11.052544	-0.077570	4.818261
391.420589	7999.888763	11.057549	-0.077590	4.818259
391.311474	7999.919862	11.062554	-0.077570	4.818269
391.296730	7999.927015	11.067559	-0.077567	4.818271
391.182447	7999.952789	11.072563	-0.077545	4.818279
391.252028	7999.902234	11.077568	-0.077558	4.818264
391.337628	7999.916000	11.082573	-0.077574	4.818268
391.422809	7999.891929	11.087578	-0.077590	4.818260
391.414648	7999.889714	11.092583	-0.077588	4.818260
391.685275	7999.914393	11.097587	-0.077639	4.818266
391.297501	7999.941718	11.102592	-0.077567	4.818275
391.187701	7999.966502	11.107597	-0.077546	4.818283
391.131009	7999.907931	11.112602	-0.077536	4.818266
391.225739	7999.910262	11.117607	-0.077553	4.818266
391.597078	7999.880606	11.122611	-0.077622	4.818256
391.602936	7999.870173	11.127616	-0.077623	4.818253
391.603942	7999.898559	11.132621	-0.077623	4.818261
391.706188	7999.864209	11.137626	-0.077642	4.818251
391.521973	7999.884832	11.142631	-0.077608	4.818258
391.880736	7999.885483	11.147635	-0.077675	4.818256
391.553087	7999.883146	11.152640	-0.077614	4.818257
391.633332	7999.914706	11.157645	-0.077629	4.818266
391.576800	7999.914988	11.162650	-0.077618	4.818266
391.258553	7999.928542	11.167655	-0.077559	4.818272
391.472320	7999.948248	11.172659	-0.077599	4.818277
391.473453	7999.903071	11.177664	-0.077599	4.818263
391.711714	7999.923109	11.182669	-0.077643	4.818268
391.734920	7999.888740	11.187674	-0.077647	4.818258
391.307710	7999.933397	11.192679	-0.077568	4.818273
391.248355	7999.969372	11.197683	-0.077557	4.818284
391.127605	7999.881560	11.202688	-0.077534	4.818258
391.665527	7999.907756	11.207693	-0.077634	4.818264
391.642935	7999.896938	11.212698	-0.077630	4.818261
391.528971	7999.891189	11.217703	-0.077609	4.818260
391.711227	7999.909417	11.222707	-0.077643	4.818264
391.667541	7999.869939	11.227712	-0.077634	4.818253
392.052303	7999.882502	11.232717	-0.077706	4.818255
391.994808	7999.865957	11.237722	-0.077695	4.818250
392.028567	7999.870615	11.242727	-0.077702	4.818251
391.754487	7999.922599	11.247731	-0.077651	4.818268
391.770528	7999.861860	11.252736	-0.077653	4.818250
392.141952	7999.987744	11.257741	-0.077723	4.818286
392.156648	7999.839759	11.262746	-0.077725	4.818242
392.198822	7999.880262	11.267751	-0.077733	4.818254
392.162180	7999.856643	11.272755	-0.077726	4.818247
391.949020	7999.861110	11.277760	-0.077686	4.818249
391.892217	7999.893967	11.282765	-0.077676	4.818259
391.678302	7999.919443	11.287770	-0.077636	4.818267
392.452898	7999.796461	11.292775	-0.077780	4.818228
392.752135	7999.932930	11.297779	-0.077836	4.818267
392.250944	7999.849420	11.302784	-0.077742	4.818244
392.323365	7999.855652	11.307789	-0.077756	4.818246
392.229516	7999.889059	11.312794	-0.077738	4.818256
392.491954	7999.857930	11.317799	-0.077787	4.818246
392.636439	7999.963928	11.322803	-0.077814	4.818277
392.512150	7999.831924	11.327808	-0.077791	4.818238
392.222164	7999.892101	11.332813	-0.077737	4.818257
392.133467	7999.898253	11.337818	-0.077720	4.818259
392.549553	7999.898631	11.342823	-0.077798	4.818258
392.880204	7999.809573	11.347827	-0.077859	4.818230
392.659369	7999.828649	11.352832	-0.077818	4.818236
392.487278	7999.888321	11.357837	-0.077786	4.818255
392.594470	7999.945470	11.362842	-0.077806	4.818271
392.473081	7999.860798	11.367847	-0.077783	4.818247
392.315595	7999.901750	11.372851	-0.077754	4.818260
392.919868	7999.811144	11.377856	-0.077866	4.818230
392.739355	7999.844428	11.382861	-0.077833	4.818241
392.766223	7999.908897	11.387866	-0.077838	4.818260
392.444237	7999.845680	11.392871	-0.077778	4.818242
392.490966	7999.909366	11.397875	-0.077786	4.818261
392.030009	7999.932546	11.402880	-0.077701	4.818270
392.370067	7999.918232	11.407885	-0.077764	4.818264
392.665327	7999.903312	11.412890	-0.077819	4.818259
392.839166	7999.863626	11.417895	-0.077851	4.818246
392.713230	7999.984878	11.422899	-0.077828	4.818283
392.588312	7999.838152	11.427904	-0.077804	4.818240
392.727968	7999.878926	11.432909	-0.077830	4.818251
392.662554	7999.849661	11.437914	-0.077818	4.818243
392.665373	7999.846544	11.442919	-0.077819	4.818242
393.007208	7999.945757	11.447923	-0.077882	4.818270
392.940690	7999.805077	11.452928	-0.077870	4.818228
392.742211	7999.919040	11.457933	-0.077833	4.818263
393.348249	7999.877854	11.462938	-0.077946	4.818248
392.926117	7999.803820	11.467943	-0.077867	4.818228
393.157077	7999.829016	11.472947	-0.077910	4.818235
392.593184	7999.845546	11.477952	-0.077805	4.818242
392.735865	7999.943112	11.482957	-0.077831	4.818270
392.683038	7999.880387	11.487962	-0.077821	4.818252
392.537166	7999.881561	11.492967	-0.077794	4.818253
393.299247	7999.861405	11.497971	-0.077936	4.818244
393.123198	7999.816979	11.502976	-0.077903	4.818231
393.099074	7999.854483	11.507981	-0.077899	4.818242
392.993938	7999.953947	11.512986	-0.077879	4.818272
392.956651	7999.852548	11.517991	-0.077872	4.818242
392.817405	7999.884289	11.522995	-0.077846	4.818252
393.098994	7999.808229	11.528000	-0.077899	4.818229
393.498222	7999.834654	11.533005	-0.077973	4.818235
392.866931	7999.967976	11.538010	-0.077855	4.818277
392.802890	7999.868316	11.543015	-0.077843	4.818248
393.002425	7999.897290	11.548019	-0.077880	4.818256
393.271914	7999.820015	11.553024	-0.077931	4.818231
392.703544	7999.873268	11.558029	-0.077825	4.818250
392.800005	7999.852502	11.563034	-0.077843	4.818243
392.793297	7999.929127	11.568039	-0.077841	4.818266
392.865734	7999.871252	11.573043	-0.077855	4.818248
392.898086	7999.828599	11.578048	-0.077861	4.818236
392.937477	7999.885881	11.583053	-0.077868	4.818252
393.191180	7999.865143	11.588058	-0.077915	4.818245
392.933657	7999.857447	11.593063	-0.077867	4.818244
393.419753	7999.937598	11.598067	-0.077958	4.818266
393.073804	7999.871952	11.603072	-0.077893	4.818248
392.933913	7999.811201	11.608077	-0.077867	4.818230
392.900504	7999.844375	11.613082	-0.077861	4.818240
392.960597	7999.892479	11.618087	-0.077872	4.818254
393.234304	7999.815261	11.623091	-0.077923	4.818230
392.751019	7999.825527	11.628096	-0.077833	4.818235
393.251502	7999.912176	11.633101	-0.077926	4.818259
393.540393	7999.898222	11.638106	-0.077980	4.818254
393.385009	7999.907674	11.643111	-0.077951	4.818257
392.995368	7999.877169	11.648115	-0.077878	4.818250
392.728157	7999.897717	11.653120	-0.077829	4.818257
393.086157	7999.846864	11.658125	-0.077895	4.818240
393.056843	7999.840159	11.663130	-0.077890	4.818238
392.948466	7999.877572	11.668135	-0.077869	4.818250
393.060613	7999.866478	11.673139	-0.077890	4.818246
392.816302	7999.946190	11.678144	-0.077845	4.818271
392.684501	7999.879243	11.683149	-0.077820	4.818251
392.639965	7999.895451	11.688154	-0.077812	4.818256
392.542400	7999.882567	11.693159	-0.077794	4.818253
393.062455	7999.879099	11.698163	-0.077890	4.818250
393.300492	7999.790889	11.703168	-0.077935	4.818223
392.946882	7999.908005	11.708173	-0.077869	4.818259
392.734035	7999.897762	11.713178	-0.077829	4.818257
392.935718	7999.866861	11.718183	-0.077867	4.818247
393.207782	7999.892614	11.723187	-0.077917	4.818253
393.140515	7999.868579	11.728192	-0.077905	4.818246
393.618202	7999.821450	11.733197	-0.077994	4.818231
393.421052	7999.937534	11.738202	-0.077957	4.818266
393.032426	7999.863953	11.743207	-0.077884	4.818246
393.519347	7999.835866	11.748211	-0.077975	4.818235
392.945729	7999.876435	11.753216	-0.077868	4.818250
392.715835	7999.923763	11.758221	-0.077825	4.818265
392.699949	7999.905679	11.763226	-0.077822	4.818259
392.438423	7999.926305	11.768231	-0.077774	4.818266
392.548593	7999.970883	11.773235	-0.077794	4.818279
392.132665	7999.935820	11.778240	-0.077717	4.818270
392.479801	7999.957334	11.783245	-0.077781	4.818275
392.768033	7999.929708	11.788250	-0.077835	4.818266
393.217071	7999.871680	11.793255	-0.077918	4.818247
393.286447	7999.894688	11.798259	-0.077931	4.818254
393.266660	7999.860786	11.803264	-0.077928	4.818244
393.514133	7999.906175	11.808269	-0.077974	4.818256
393.062775	7999.851712	11.813274	-0.077890	4.818242
393.341304	7999.856534	11.818279	-0.077941	4.818242
393.080122	7999.943374	11.823283	-0.077893	4.818269
393.189083	7999.861822	11.828288	-0.077913	4.818244
393.367858	7999.878955	11.833293	-0.077946	4.818249
393.192629	7999.959603	11.838298	-0.077914	4.818273
392.657287	7999.925022	11.843303	-0.077814	4.818265
392.552305	7999.972992	11.848307	-0.077794	4.818280
392.854186	7999.907716	11.853312	-0.077850	4.818259
392.761909	7999.941144	11.858317	-0.077833	4.818270
392.877549	7999.904874	11.863322	-0.077855	4.818258
392.929685	7999.883507	11.868327	-0.077864	4.818252
393.480857	7999.874157	11.873331	-0.077967	4.818247
393.477884	7999.819464	11.878336	-0.077966	4.818231
393.448293	7999.862150	11.883341	-0.077961	4.818243
393.472023	7999.880335	11.888346	-0.077965	4.818249
393.754796	7999.892572	11.893351	-0.078018	4.818251
393.369856	7999.933594	11.898355	-0.077946	4.818265
393.640331	7999.874199	11.903360	-0.077996	4.818246
394.150995	7999.911596	11.908365	-0.078091	4.818255
393.663990	7999.876616	11.913370	-0.078001	4.818247
393.527635	7999.861102	11.918375	-0.077975	4.818243
393.795416	7999.875238	11.923379	-0.078025	4.818246
393.350136	7999.888118	11.928384	-0.077942	4.818251
393.152814	7999.895951	11.933389	-0.077905	4.818255
393.474565	7999.849862	11.938394	-0.077965	4.818240
393.585994	7999.909172	11.943399	-0.077986	4.818257
393.643233	7999.866855	11.948403	-0.077997	4.818244
393.717113	7999.785879	11.953408	-0.078010	4.818220
393.625157	7999.929663	11.958413	-0.077993	4.818263
393.432399	7999.860837	11.963418	-0.077957	4.818243
393.506787	7999.821905	11.968423	-0.077971	4.818231
393.635947	7999.867793	11.973427	-0.077995	4.818244
393.943268	7999.902434	11.978432	-0.078052	4.818253
393.903562	7999.840936	11.983437	-0.078045	4.818235
393.662281	7999.893364	11.988442	-0.078000	4.818252
394.077397	7999.766566	11.993447	-0.078077	4.818212
394.364170	7999.886057	11.998451	-0.078130	4.818247
394.179569	7999.971834	12.003456	-0.078096	4.818273
394.076819	7999.801231	12.008461	-0.078077	4.818223
393.653906	7999.853300	12.013466	-0.077998	4.818240
393.915288	7999.996619	12.018471	-0.078047	4.818281
394.158640	7999.842268	12.023475	-0.078092	4.818235
393.644042	7999.854208	12.028480	-0.077996	4.818240
393.667896	7999.889211	12.033485	-0.078001	4.818251
393.951718	7999.863627	12.038490	-0.078053	4.818242
393.835091	7999.877808	12.043495	-0.078032	4.818246
393.756885	7999.970282	12.048499	-0.078017	4.818274
394.017765	7999.845596	12.053504	-0.078065	4.818236
394.419898	7999.895186	12.058509	-0.078140	4.818249
394.368871	7999.774679	12.063514	-0.078131	4.818214
394.306062	7999.944084	12.068519	-0.078119	4.818264
394.532842	7999.846261	12.073523	-0.078161	4.818234
394.372929	7999.839886	12.078528	-0.078131	4.818233
394.460352	7999.751735	12.083533	-0.078148	4.818206
394.282454	7999.891203	12.088538	-0.078114	4.818249
393.556264	7999.869796	12.093543	-0.077979	4.818245
393.789613	7999.863497	12.098547	-0.078023	4.818242
393.732396	7999.850107	12.103552	-0.078012	4.818239
394.013512	7999.939043	12.108557	-0.078064	4.818264
393.933320	7999.865436	12.113562	-0.078049	4.818242
394.016730	7999.823474	12.118567	-0.078065	4.818230
393.839520	7999.893586	12.123571	-0.078032	4.818251
393.562172	7999.868805	12.128576	-0.077980	4.818245
393.159257	7999.895922	12.133581	-0.077905	4.818255
393.019940	7999.925560	12.138586	-0.077879	4.818264
393.019725	7999.928707	12.143591	-0.077879	4.818265
393.044616	7999.906972	12.148595	-0.077884	4.818258
393.056562	7999.886111	12.153600	-0.077886	4.818252
392.871741	7999.915133	12.158605	-0.077851	4.818261
392.952553	7999.919378	12.163610	-0.077866	4.818262
392.802749	7999.921549	12.168615	-0.077838	4.818264
392.652064	7999.973103	12.173619	-0.077810	4.818280
392.553550	7999.969664	12.178624	-0.077792	4.818279
392.509923	7999.935440	12.183629	-0.077784	4.818269
392.772487	7999.935841	12.188634	-0.077833	4.818268
392.657322	7999.929023	12.193639	-0.077811	4.818266
392.952085	7999.921453	12.198643	-0.077866	4.818263
392.981701	7999.874559	12.203648	-0.077871	4.818249
393.194095	7999.897401	12.208653	-0.077911	4.818255
393.300011	7999.899885	12.213658	-0.077931	4.818255
393.463552	7999.875824	12.218663	-0.077961	4.818247
393.463152	7999.984065	12.223667	-0.077961	4.818280
393.213419	7999.846155	12.228672	-0.077914	4.818240
393.059912	7999.888212	12.233677	-0.077886	4.818253
393.448221	7999.875605	12.238682	-0.077958	4.818247
393.120515	7999.866957	12.243687	-0.077897	4.818246
393.897158	7999.855409	12.248691	-0.078041	4.818240
393.519805	7999.839782	12.253696	-0.077971	4.818236
393.761254	7999.854612	12.258701	-0.078016	4.818240
394.088360	7999.910540	12.263706	-0.078077	4.818255
393.650270	7999.829981	12.268711	-0.077995	4.818233
393.852068	7999.841120	12.273715	-0.078033	4.818236
393.942346	7999.918011	12.278720	-0.078050	4.818258
393.720313	7999.867705	12.283725	-0.078008	4.818244
393.622944	7999.873739	12.288730	-0.077990	4.818246
393.987824	7999.848204	12.293735	-0.078058	4.818237
394.062798	7999.858676	12.298739	-0.078072	4.818240
393.838471	7999.872448	12.303744	-0.078030	4.818245
394.047340	7999.839543	12.308749	-0.078069	4.818234
394.361209	7999.904751	12.313754	-0.078127	4.818252
393.751814	7999.844990	12.318759	-0.078014	4.818237
393.069968	7999.938742	12.323763	-0.077887	4.818268
393.266700	7999.915131	12.328768	-0.077923	4.818260
392.955396	7999.936133	12.333773	-0.077865	4.818267
393.051575	7999.958452	12.338778	-0.077883	4.818274
393.144908	7999.940797	12.343783	-0.077901	4.818268
393.320037	7999.929504	12.348787	-0.077933	4.818264
393.455276	7999.885092	12.353792	-0.077958	4.818250
393.323217	7999.929542	12.358797	-0.077934	4.818264
393.390913	7999.960934	12.363802	-0.077946	4.818273
393.662072	7999.878427	12.368807	-0.077997	4.818247
393.299450	7999.935517	12.373811	-0.077929	4.818266
393.320364	7999.942103	12.378816	-0.077933	4.818268
393.212290	7999.982674	12.383821	-0.077913	4.818280
392.872203	8000.008540	12.388826	-0.077850	4.818289
392.810055	7999.966708	12.393831	-0.077838	4.818277
393.334465	7999.961200	12.398835	-0.077936	4.818273
393.509216	7999.893150	12.403840	-0.077968	4.818252
393.503391	7999.904629	12.408845	-0.077967	4.818256
393.516762	7999.925827	12.413850	-0.077969	4.818262
393.463024	7999.898821	12.418855	-0.077959	4.818254
393.533721	7999.918694	12.423859	-0.077972	4.818260
393.381160	7999.892452	12.428864	-0.077944	4.818253
393.764142	7999.852447	12.433869	-0.078015	4.818239
394.115198	7999.831979	12.438874	-0.078081	4.818232
393.668212	7999.867957	12.443879	-0.077997	4.818244
393.867101	7999.924249	12.448883	-0.078034	4.818260
394.104616	7999.910650	12.453888	-0.078078	4.818255
394.235952	7999.813636	12.458893	-0.078103	4.818226
394.345565	7999.860311	12.463898	-0.078123	4.818239
393.969722	7999.937189	12.468903	-0.078053	4.818264
393.632998	7999.945234	12.473907	-0.077991	4.818267
393.501380	7999.916122	12.478912	-0.077966	4.818259
394.070042	7999.879686	12.483917	-0.078072	4.818246
394.553116	7999.843141	12.488922	-0.078162	4.818233
394.403943	7999.836912	12.493927	-0.078134	4.818232
394.493869	7999.849689	12.498931	-0.078151	4.818236
394.255534	7999.921075	12.503936	-0.078106	4.818258
394.331991	7999.829622	12.508941	-0.078120	4.818230
394.260634	7999.866487	12.513946	-0.078107	4.818241
394.790859	7999.786441	12.518951	-0.078206	4.818216
394.689676	7999.961633	12.523955	-0.078187	4.818268
395.132556	7999.761640	12.528960	-0.078269	4.818207
394.660697	7999.830911	12.533965	-0.078181	4.818229
394.218164	7999.859591	12.538970	-0.078099	4.818240
394.025896	7999.957876	12.543975	-0.078063	4.818270
394.153757	7999.873426	12.548979	-0.078087	4.818244
393.720247	7999.891719	12.553984	-0.078006	4.818251
393.700957	7999.910372	12.558989	-0.078002	4.818257
394.088764	7999.891454	12.563994	-0.078075	4.818250
393.901353	7999.859483	12.568999	-0.078040	4.818241
394.003251	7999.879779	12.574003	-0.078059	4.818246
393.570586	7999.881269	12.579008	-0.077978	4.818249
393.347964	7999.939205	12.584013	-0.077937	4.818267
393.835287	7999.878544	12.589018	-0.078027	4.818247
393.403682	7999.898966	12.594023	-0.077947	4.818255
393.738831	7999.909811	12.599027	-0.078009	4.818256
394.190588	7999.823446	12.604032	-0.078093	4.818229
394.344057	7999.914857	12.609037	-0.078122	4.818256
394.311035	7999.837685	12.614042	-0.078116	4.818233
394.104340	7999.933672	12.619047	-0.078077	4.818262
393.986329	7999.908948	12.624051	-0.078055	4.818255
393.842639	7999.900691	12.629056	-0.078028	4.818253
393.660145	7999.916081	12.634061	-0.077994	4.818259
393.615713	7999.924935	12.639066	-0.077986	4.818261
393.857350	7999.878811	12.644071	-0.078031	4.818247
394.020915	7999.937778	12.649075	-0.078061	4.818264
393.649413	7999.897007	12.654080	-0.077992	4.818253
393.821399	7999.907743	12.659085	-0.078024	4.818256
393.945608	7999.908372	12.664090	-0.078047	4.818255
393.660148	7999.910806	12.669095	-0.077994	4.818257
393.368438	7999.977264	12.674099	-0.077940	4.818278
393.845432	7999.925923	12.679104	-0.078028	4.818261
394.377962	7999.891100	12.684109	-0.078128	4.818248
394.167557	7999.916621	12.689114	-0.078088	4.818257
393.958566	7999.912734	12.694119	-0.078049	4.818256
394.353597	7999.918087	12.699123	-0.078123	4.818256
394.049481	7999.868769	12.704128	-0.078066	4.818243
393.843939	7999.912223	12.709133	-0.078028	4.818257
393.786878	7999.944027	12.714138	-0.078017	4.818266
394.363167	7999.824668	12.719143	-0.078124	4.818229
393.959973	7999.893819	12.724147	-0.078049	4.818251
393.806905	7999.885435	12.729152	-0.078021	4.818249
394.115333	7999.903276	12.734157	-0.078078	4.818253
393.861063	7999.864093	12.739162	-0.078031	4.818242
393.094069	7999.966149	12.744167	-0.077888	4.818276
393.196513	7999.972789	12.749171	-0.077907	4.818277
393.492637	7999.943168	12.754176	-0.077962	4.818267
393.660805	7999.951750	12.759181	-0.077993	4.818269
393.973348	7999.939169	12.764186	-0.078052	4.818264
393.510274	7999.975979	12.769191	-0.077965	4.818277
393.672488	7999.993939	12.774195	-0.077996	4.818282
393.413471	8000.038770	12.779200	-0.077947	4.818296
393.457105	7999.968943	12.784205	-0.077955	4.818275
393.465218	7999.995325	12.789210	-0.077957	4.818283
393.213268	8000.004519	12.794215	-0.077910	4.818287
393.361064	8000.040150	12.799219	-0.077937	4.818297
393.396361	7999.927121	12.804224	-0.077944	4.818263
393.519391	7999.927734	12.809229	-0.077967	4.818263
393.565321	7999.950424	12.814234	-0.077975	4.818269
393.902241	7999.911898	12.819239	-0.078038	4.818256
393.632651	7999.946076	12.824243	-0.077988	4.818268
393.786357	7999.932392	12.829248	-0.078016	4.818263
393.917113	7999.956232	12.834253	-0.078041	4.818270
393.789971	7999.988137	12.839258	-0.078017	4.818280
393.707955	7999.956544	12.844263	-0.078002	4.818270
393.358279	8000.042185	12.849267	-0.077936	4.818297
393.565352	8000.013460	12.854272	-0.077975	4.818288
393.558361	7999.991292	12.859277	-0.077974	4.818281
393.897544	8000.002192	12.864282	-0.078037	4.818283
393.629814	7999.976490	12.869287	-0.077987	4.818277
393.693099	8000.025689	12.874291	-0.077999	4.818291
393.523670	7999.983453	12.879296	-0.077967	4.818279
394.009691	7999.920674	12.884301	-0.078057	4.818259
394.174537	7999.950231	12.889306	-0.078088	4.818267
393.786053	7999.918687	12.894311	-0.078016	4.818259
393.549897	8000.003765	12.899315	-0.077972	4.818285
393.713084	7999.946069	12.904320	-0.078002	4.818267
393.548490	7999.959600	12.909325	-0.077971	4.818272
393.816847	7999.966387	12.914330	-0.078021	4.818273
393.783304	7999.955420	12.919335	-0.078015	4.818270
394.125977	7999.934839	12.924339	-0.078079	4.818262
394.468752	7999.862761	12.929344	-0.078142	4.818240
394.136843	7999.977019	12.934349	-0.078081	4.818275
393.846719	7999.964675	12.939354	-0.078027	4.818272
393.906192	7999.905573	12.944359	-0.078038	4.818255
393.837886	7999.968754	12.949363	-0.078025	4.818274
394.294612	7999.915037	12.954368	-0.078110	4.818256
394.191827	7999.911538	12.959373	-0.078091	4.818255
394.409460	7999.881905	12.964378	-0.078131	4.818246
394.563755	7999.887147	12.969383	-0.078160	4.818246
394.474165	7999.923765	12.974387	-0.078143	4.818258
394.124191	7999.907457	12.979392	-0.078078	4.818254
394.516538	7999.886499	12.984397	-0.078151	4.818246
394.231934	7999.950951	12.989402	-0.078098	4.818267
394.720343	7999.841962	12.994407	-0.078189	4.818232
395.070590	7999.798362	12.999411	-0.078254	4.818218
394.882066	7999.919820	13.004416	-0.078219	4.818255
394.630778	7999.874370	13.009421	-0.078172	4.818242
394.696056	7999.885762	13.014426	-0.078184	4.818246
394.509406	7999.868515	13.019431	-0.078149	4.818241
394.606213	7999.868773	13.024435	-0.078167	4.818241
394.992183	7999.798332	13.029440	-0.078239	4.818218
394.922040	7999.929804	13.034445	-0.078226	4.818258
395.096293	7999.861747	13.039450	-0.078258	4.818237
394.937341	7999.910037	13.044455	-0.078229	4.818252
394.704674	7999.881655	13.049459	-0.078185	4.818244
394.607862	7999.885594	13.054464	-0.078167	4.818246
394.543306	7999.873155	13.059469	-0.078155	4.818242
394.288093	7999.901221	13.064474	-0.078108	4.818252
394.006359	7999.939438	13.069479	-0.078055	4.818264
394.397033	7999.932120	13.074483	-0.078128	4.818261
394.203824	7999.880102	13.079488	-0.078092	4.818246
393.896025	7999.932679	13.084493	-0.078035	4.818263
393.837080	7999.956050	13.089498	-0.078024	4.818270
393.696676	7999.944685	13.094503	-0.077997	4.818267
394.300190	7999.928691	13.099507	-0.078110	4.818260
394.011866	7999.933187	13.104512	-0.078056	4.818262
394.149664	7999.921389	13.109517	-0.078082	4.818258
394.356428	7999.928393	13.114522	-0.078120	4.818260
393.949259	7999.913412	13.119527	-0.078044	4.818257
394.208829	7999.990497	13.124531	-0.078093	4.818279
394.350003	7999.927247	13.129536	-0.078119	4.818259
394.004023	7999.982459	13.134541	-0.078054	4.818277
394.281593	7999.984118	13.139546	-0.078106	4.818276
394.237977	7999.924668	13.144551	-0.078098	4.818259
394.045192	7999.953581	13.149555	-0.078062	4.818268
393.989073	7999.970684	13.154560	-0.078051	4.818274
394.200839	7999.940972	13.159565	-0.078091	4.818264
393.986422	7999.967489	13.164570	-0.078051	4.818273
394.081685	7999.922535	13.169575	-0.078068	4.818259
394.506484	7999.933546	13.174579	-0.078148	4.818261
394.572412	7999.878735	13.179584	-0.078160	4.818244
394.459470	7999.925546	13.184589	-0.078139	4.818258
394.511353	7999.938858	13.189594	-0.078148	4.818262
394.052927	7999.965220	13.194599	-0.078063	4.818272
394.052140	7999.989379	13.199603	-0.078063	4.818279
393.918299	7999.966542	13.204608	-0.078038	4.818273
393.936918	7999.947874	13.209613	-0.078041	4.818267
393.871433	7999.991125	13.214618	-0.078029	4.818280
393.694011	7999.949831	13.219623	-0.077996	4.818269
394.028093	7999.958560	13.224627	-0.078058	4.818270
394.248912	7999.886931	13.229632	-0.078099	4.818248
394.231390	7999.924526	13.234637	-0.078096	4.818259
394.358169	7999.961976	13.239642	-0.078119	4.818270
394.158283	7999.961365	13.244647	-0.078082	4.818270
394.307654	7999.981254	13.249651	-0.078110	4.818275
394.110942	7999.986992	13.254656	-0.078073	4.818278
393.994388	7999.980154	13.259661	-0.078052	4.818276
393.895642	7999.983016	13.264666	-0.078033	4.818278
394.010380	7999.935173	13.269671	-0.078054	4.818263
394.335537	7999.956394	13.274675	-0.078115	4.818268
394.422699	7999.935502	13.279680	-0.078131	4.818261
394.432692	7999.926175	13.284685	-0.078133	4.818259
394.385294	7999.966518	13.289690	-0.078124	4.818271
394.385340	7999.895049	13.294695	-0.078124	4.818250
394.538206	7999.911833	13.299699	-0.078152	4.818254
394.620791	7999.896134	13.304704	-0.078168	4.818249
394.190093	7999.941790	13.309709	-0.078088	4.818264
394.520284	7999.909479	13.314714	-0.078149	4.818253
394.411058	7999.964748	13.319719	-0.078129	4.818270
394.655068	7999.869261	13.324723	-0.078174	4.818241
394.357385	7999.928281	13.329728	-0.078119	4.818260
394.762239	7999.806598	13.334733	-0.078194	4.818222
394.554531	7999.907827	13.339738	-0.078155	4.818253
394.551451	7999.890966	13.344743	-0.078155	4.818248
395.342766	7999.849144	13.349747	-0.078302	4.818232
394.558477	7999.922585	13.354752	-0.078156	4.818257
394.476209	7999.933028	13.359757	-0.078140	4.818261
394.653014	7999.936473	13.364762	-0.078173	4.818261
394.106212	7999.935362	13.369767	-0.078071	4.818263
394.272087	7999.955475	13.374771	-0.078102	4.818268
394.085087	7999.963447	13.379776	-0.078067	4.818271
394.311511	7999.937086	13.384781	-0.078110	4.818262
394.497344	7999.943807	13.389786	-0.078144	4.818264
394.531851	7999.884365	13.394791	-0.078150	4.818246
394.379415	7999.942202	13.399795	-0.078122	4.818264
394.497665	7999.916477	13.404800	-0.078144	4.818256
394.554359	7999.887815	13.409805	-0.078155	4.818247
394.976409	7999.875668	13.414810	-0.078233	4.818241
394.477122	7999.892017	13.419815	-0.078140	4.818248
395.024268	7999.962493	13.424819	-0.078242	4.818267
395.213290	7999.851546	13.429824	-0.078277	4.818233
395.409097	7999.815311	13.434829	-0.078313	4.818222
395.148929	7999.896911	13.439834	-0.078265	4.818247
395.522053	7999.851521	13.444839	-0.078334	4.818232
395.364864	7999.905089	13.449843	-0.078305	4.818249
394.971531	7999.844049	13.454848	-0.078232	4.818232
395.065640	7999.836914	13.459853	-0.078249	4.818230
395.458871	7999.847499	13.464858	-0.078323	4.818231
395.297067	7999.894699	13.469863	-0.078292	4.818246
395.167437	7999.874020	13.474867	-0.078268	4.818240
394.864972	7999.891986	13.479872	-0.078212	4.818247
394.458527	7999.916950	13.484877	-0.078136	4.818256
394.404928	7999.947750	13.489882	-0.078126	4.818265
394.540148	7999.901235	13.494887	-0.078151	4.818251
394.816473	7999.914438	13.499891	-0.078203	4.818254
394.731801	7999.900675	13.504896	-0.078187	4.818250
394.925474	7999.905401	13.509901	-0.078223	4.818251
394.641717	7999.967763	13.514906	-0.078170	4.818270
394.288164	7999.926181	13.519911	-0.078104	4.818259
394.294715	7999.942032	13.524915	-0.078105	4.818264
394.544689	7999.939112	13.529920	-0.078152	4.818262
394.188813	7999.984731	13.534925	-0.078086	4.818277
394.387900	7999.962204	13.539930	-0.078123	4.818270
394.263585	7999.957363	13.544935	-0.078099	4.818269
394.304840	7999.975786	13.549939	-0.078107	4.818274
394.167437	7999.952900	13.554944	-0.078081	4.818268
393.906921	7999.976691	13.559949	-0.078033	4.818276
394.163727	7999.952844	13.564954	-0.078081	4.818268
394.144579	7999.960990	13.569959	-0.078077	4.818270
394.459421	7999.965256	13.574963	-0.078136	4.818270
394.805921	7999.921606	13.579968	-0.078200	4.818256
394.800652	7999.901562	13.584973	-0.078199	4.818250
394.901700	7999.925001	13.589978	-0.078218	4.818256
394.815615	7999.866026	13.594983	-0.078202	4.818239
395.036220	7999.907901	13.599987	-0.078243	4.818251
394.689297	7999.948386	13.604992	-0.078178	4.818264
394.356402	7999.962787	13.609997	-0.078116	4.818270
394.530283	7999.948326	13.615002	-0.078148	4.818265
394.360399	7999.923949	13.620007	-0.078117	4.818258
394.453633	7999.942026	13.625011	-0.078134	4.818263
394.759843	7999.912544	13.630016	-0.078191	4.818253
394.509784	7999.942782	13.635021	-0.078144	4.818263
394.754379	7999.919821	13.640026	-0.078190	4.818256
394.737013	7999.882798	13.645031	-0.078187	4.818245
394.368187	7999.960822	13.650035	-0.078118	4.818269
394.344756	7999.949991	13.655040	-0.078114	4.818266
394.581705	7999.985782	13.660045	-0.078158	4.818276
394.834275	7999.907227	13.665050	-0.078205	4.818251
394.528611	7999.881008	13.670055	-0.078148	4.818245
394.916364	7999.907283	13.675059	-0.078220	4.818251
394.910972	7999.892493	13.680064	-0.078219	4.818247
394.833161	7999.901945	13.685069	-0.078204	4.818250
394.841707	7999.902058	13.690074	-0.078206	4.818250
394.939336	7999.877104	13.695079	-0.078224	4.818242
394.882713	7999.925730	13.700083	-0.078213	4.818257
394.720329	7999.906709	13.705088	-0.078183	4.818252
394.636065	7999.888748	13.710093	-0.078167	4.818247
394.932974	7999.904332	13.715098	-0.078223	4.818250
394.828204	7999.883990	13.720103	-0.078203	4.818245
394.812955	7999.871169	13.725107	-0.078200	4.818241
394.936672	7999.854977	13.730112	-0.078223	4.818236
395.082013	7999.941025	13.735117	-0.078250	4.818261
395.078058	7999.867398	13.740122	-0.078249	4.818239
395.277282	7999.828057	13.745127	-0.078286	4.818226
395.222046	7999.899824	13.750131	-0.078276	4.818248
395.217854	7999.878744	13.755136	-0.078275	4.818241
395.218294	7999.881900	13.760141	-0.078275	4.818242
395.757598	7999.857682	13.765146	-0.078376	4.818233
395.740900	7999.779678	13.770151	-0.078373	4.818210
395.609135	7999.919775	13.775155	-0.078348	4.818252
395.021952	7999.876073	13.780160	-0.078239	4.818241
395.789153	7999.874915	13.785165	-0.078381	4.818238
395.094977	7999.921199	13.790170	-0.078252	4.818255
395.071701	7999.880943	13.795175	-0.078248	4.818243
395.188023	7999.904589	13.800179	-0.078269	4.818249
395.329206	7999.868664	13.805184	-0.078296	4.818238
394.862995	7999.895971	13.810189	-0.078209	4.818248
394.903425	7999.948015	13.815194	-0.078216	4.818263
394.839460	7999.871473	13.820199	-0.078204	4.818241
394.986986	7999.901847	13.825203	-0.078232	4.818249
395.193304	7999.894133	13.830208	-0.078270	4.818246
395.046372	7999.928922	13.835213	-0.078243	4.818257
395.164390	7999.902143	13.840218	-0.078265	4.818249
395.394326	7999.837994	13.845223	-0.078307	4.818229
394.962563	7999.896247	13.850227	-0.078227	4.818248
394.933835	7999.984138	13.855232	-0.078222	4.818274
395.154331	7999.885179	13.860237	-0.078263	4.818244
395.140904	7999.928085	13.865242	-0.078260	4.818256
394.946894	7999.932808	13.870247	-0.078224	4.818259
395.058676	7999.898587	13.875251	-0.078245	4.818248
395.369887	7999.825030	13.880256	-0.078303	4.818225
395.254151	7999.853937	13.885261	-0.078281	4.818234
395.248545	7999.885388	13.890266	-0.078280	4.818243
394.885113	7999.859436	13.895271	-0.078212	4.818237
395.442213	7999.855428	13.900275	-0.078316	4.818234
395.533552	7999.913418	13.905280	-0.078333	4.818251
394.910983	7999.890257	13.910285	-0.078217	4.818246
395.026564	7999.923352	13.915290	-0.078238	4.818256
395.081887	7999.874702	13.920295	-0.078249	4.818241
394.884635	7999.922472	13.925299	-0.078212	4.818256
394.686797	7999.935551	13.930304	-0.078175	4.818261
395.215417	7999.924851	13.935309	-0.078273	4.818255
395.516349	7999.936287	13.940314	-0.078329	4.818257
395.247453	7999.891647	13.945319	-0.078279	4.818245
395.155742	7999.950308	13.950323	-0.078262	4.818263
395.281609	7999.888952	13.955328	-0.078286	4.818244
394.906065	7999.895416	13.960333	-0.078216	4.818248
394.974996	7999.911062	13.965338	-0.078228	4.818252
395.101531	7999.875990	13.970343	-0.078252	4.818241
395.410915	7999.867572	13.975347	-0.078310	4.818237
395.331404	7999.861235	13.980352	-0.078295	4.818236
395.527831	7999.857591	13.985357	-0.078331	4.818234
395.360983	7999.908926	13.990362	-0.078300	4.818250
395.075109	7999.887179	13.995367	-0.078247	4.818245
395.544491	7999.885134	14.000371	-0.078334	4.818242
395.370557	7999.977363	14.005376	-0.078302	4.818270
395.055246	7999.900563	14.010381	-0.078243	4.818249
395.130363	7999.915242	14.015386	-0.078257	4.818253
395.405693	7999.868526	14.020391	-0.078308	4.818238
395.513263	7999.877339	14.025395	-0.078328	4.818240
395.696420	7999.810454	14.030400	-0.078362	4.818219
395.753902	7999.885852	14.035405	-0.078373	4.818241
395.506541	7999.916126	14.040410	-0.078327	4.818251
395.471165	7999.845226	14.045415	-0.078320	4.818231
395.487298	7999.937931	14.050419	-0.078323	4.818258
395.715089	7999.850631	14.055424	-0.078366	4.818231
395.615463	7999.850327	14.060429	-0.078347	4.818231
395.722554	7999.846522	14.065434	-0.078367	4.818230
395.759800	7999.910085	14.070439	-0.078374	4.818249
395.266194	7999.860295	14.075443	-0.078282	4.818236
395.341854	7999.831891	14.080448	-0.078296	4.818227
395.719020	7999.911625	14.085453	-0.078366	4.818249
395.461493	7999.845068	14.090458	-0.078318	4.818231
396.085082	7999.789413	14.095463	-0.078434	4.818211
395.998202	7999.904894	14.100467	-0.078418	4.818246
395.268321	7999.867664	14.105472	-0.078282	4.818238
395.092769	7999.868433	14.110477	-0.078249	4.818239
395.400059	7999.889414	14.115482	-0.078306	4.818244
395.095898	7999.890541	14.120487	-0.078250	4.818246
394.934208	7999.965068	14.125491	-0.078220	4.818268
395.015607	7999.898905	14.130496	-0.078235	4.818248
395.323047	7999.914633	14.135501	-0.078292	4.818252
395.254890	7999.950491	14.140506	-0.078279	4.818263
395.075205	7999.949102	14.145511	-0.078246	4.818263
394.957491	7999.929635	14.150515	-0.078224	4.818258
395.321750	7999.901992	14.155520	-0.078292	4.818248
395.403877	7999.874725	14.160525	-0.078307	4.818240
395.508322	7999.916078	14.165530	-0.078326	4.818251
395.131736	7999.913069	14.170535	-0.078256	4.818252
395.262419	7999.890665	14.175539	-0.078280	4.818245
395.407280	7999.971453	14.180544	-0.078307	4.818268
395.622771	7999.850354	14.185549	-0.078347	4.818231
395.898647	7999.864603	14.190554	-0.078399	4.818235
395.523125	7999.872118	14.195559	-0.078329	4.818238
395.226315	7999.891212	14.200563	-0.078273	4.818245
394.975925	7999.948771	14.205568	-0.078227	4.818263
394.997896	7999.922791	14.210573	-0.078231	4.818256
395.240234	7999.893494	14.215578	-0.078276	4.818246
395.526724	7999.846928	14.220583	-0.078329	4.818231
395.292465	7999.936237	14.225587	-0.078286	4.818258
395.765714	7999.892205	14.230592	-0.078374	4.818243
395.413019	7999.867449	14.235597	-0.078308	4.818237
395.678669	7999.906784	14.240602	-0.078357	4.818248
395.587753	7999.880323	14.245607	-0.078340	4.818241
395.413129	7999.885309	14.250611	-0.078308	4.818243
395.557889	7999.957687	14.255616	-0.078335	4.818264
395.579689	7999.823450	14.260621	-0.078339	4.818224
395.890758	7999.880218	14.265626	-0.078397	4.818239
395.703368	7999.932326	14.270631	-0.078362	4.818256
395.519640	7999.896198	14.275635	-0.078327	4.818246
395.654234	7999.841266	14.280640	-0.078352	4.818229
395.678723	7999.852105	14.285645	-0.078357	4.818232
395.858953	7999.857701	14.290650	-0.078390	4.818233
395.350838	7999.873927	14.295655	-0.078296	4.818240
395.152836	7999.911177	14.300659	-0.078259	4.818251
395.317786	7999.911309	14.305664	-0.078290	4.818251
395.113510	7999.907485	14.310669	-0.078251	4.818251
395.015390	7999.933477	14.315674	-0.078233	4.818259
394.905846	7999.922530	14.320679	-0.078213	4.818256
395.539357	7999.936375	14.325683	-0.078331	4.818257
395.429446	7999.925422	14.330688	-0.078310	4.818255
395.173178	7999.888311	14.335693	-0.078262	4.818245
395.237890	7999.896542	14.340698	-0.078274	4.818247
395.255751	7999.907292	14.345703	-0.078278	4.818250
395.165333	7999.933389	14.350707	-0.078261	4.818258
395.358200	7999.906573	14.355712	-0.078297	4.818249
395.537212	7999.945784	14.360717	-0.078330	4.818260
395.504203	7999.916956	14.365722	-0.078324	4.818252
395.662244	7999.847628	14.370727	-0.078353	4.818231
395.646981	7999.875796	14.375731	-0.078350	4.818239
395.860509	7999.844006	14.380736	-0.078390	4.818229
395.668086	7999.851903	14.385741	-0.078354	4.818232
395.710391	7999.892412	14.390746	-0.078362	4.818244
395.688123	7999.863730	14.395751	-0.078358	4.818235
395.711367	7999.639127	14.400755	-0.078362	4.818168

396.031269	7996.476037	14.405760	-0.078419	4.817227
396.457713	7990.762175	14.410765	-0.078495	4.815528
396.167519	7984.130375	14.415770	-0.078437	4.813558
395.825550	7976.834255	14.420775	-0.078368	4.811389
396.241475	7969.141102	14.425779	-0.078441	4.809098
395.817422	7961.486990	14.430784	-0.078357	4.806821
395.071499	7953.487872	14.435789	-0.078212	4.804442
395.325936	7945.660288	14.440794	-0.078255	4.802109
395.277010	7937.574164	14.445799	-0.078240	4.799698
395.119654	7929.591302	14.450803	-0.078206	4.797317
395.297984	7921.569320	14.455808	-0.078234	4.794923
395.117360	7913.602574	14.460813	-0.078195	4.792545
394.808908	7905.630060	14.465818	-0.078132	4.790164
394.717038	7897.567957	14.470823	-0.078110	4.787755
395.235063	7889.461276	14.475827	-0.078201	4.785329
395.248069	7881.614979	14.480832	-0.078198	4.782982
394.513055	7873.635377	14.485837	-0.078056	4.780596
394.593375	7865.628848	14.490842	-0.078066	4.778198
394.518932	7857.572667	14.495847	-0.078047	4.775784
394.781103	7849.556211	14.500851	-0.078090	4.773380
394.325202	7841.562736	14.505856	-0.078000	4.770984
394.520694	7833.509979	14.510861	-0.078031	4.768567
394.492396	7825.555831	14.515866	-0.078021	4.766179
394.577333	7817.435279	14.520871	-0.078031	4.763739
394.440597	7809.631557	14.525875	-0.078000	4.761394
394.519584	7801.549209	14.530880	-0.078010	4.758964
394.757413	7793.519015	14.535885	-0.078049	4.756548
394.452653	7785.517314	14.540890	-0.077987	4.754140
393.918973	7777.604983	14.545895	-0.077882	4.751758
394.186232	7769.489824	14.550899	-0.077927	4.749313
394.306210	7761.499780	14.555904	-0.077944	4.746904
394.490180	7753.355908	14.560909	-0.077973	4.744447
395.072047	7745.497368	14.565914	-0.078076	4.742074
394.460421	7737.481978	14.570919	-0.077957	4.739656
394.462349	7729.507256	14.575923	-0.077952	4.737247
394.464527	7721.521109	14.580928	-0.077947	4.734833
394.004873	7713.596883	14.585933	-0.077856	4.732438
393.858245	7705.535464	14.590938	-0.077824	4.729999
393.760187	7697.519816	14.595943	-0.077800	4.727573
393.558025	7689.501517	14.600947	-0.077757	4.725145
393.908703	7681.512287	14.605952	-0.077817	4.722724
393.910463	7673.480787	14.610957	-0.077812	4.720289
393.772117	7665.530880	14.615962	-0.077781	4.717878
393.491698	7657.483560	14.620967	-0.077724	4.715436
393.688079	7649.491254	14.625971	-0.077755	4.713009
393.627118	7641.550033	14.630976	-0.077739	4.710597
393.441343	7633.445972	14.635981	-0.077699	4.708134
393.456452	7625.522639	14.640986	-0.077696	4.705724
393.291478	7617.553354	14.645991	-0.077660	4.703300
392.582977	7609.603454	14.650995	-0.077523	4.700880
392.800938	7601.568291	14.656000	-0.077559	4.698433
392.513900	7593.510788	14.661005	-0.077500	4.695978
392.851313	7585.501781	14.666010	-0.077557	4.693535
392.730434	7577.501440	14.671015	-0.077530	4.691095
392.644017	7569.453273	14.676019	-0.077508	4.688638
392.470359	7561.524602	14.681024	-0.077471	4.686217
392.164385	7553.473073	14.686029	-0.077408	4.683757
392.062486	7545.581609	14.691034	-0.077384	4.681345
392.318904	7537.457337	14.696039	-0.077427	4.678860
392.348545	7529.543844	14.701043	-0.077427	4.676438
392.350774	7521.468233	14.706048	-0.077422	4.673966
392.170816	7513.415941	14.711053	-0.077383	4.671499
392.197511	7505.438567	14.716058	-0.077383	4.669054
392.087536	7497.414294	14.721063	-0.077357	4.666593
391.996136	7489.397379	14.726067	-0.077335	4.664133
391.764977	7481.557435	14.731072	-0.077287	4.661726
391.689429	7473.435206	14.736077	-0.077267	4.659232
392.001050	7465.459782	14.741082	-0.077320	4.656781
391.768309	7457.450666	14.746087	-0.077272	4.654318
391.816284	7449.493631	14.751091	-0.077275	4.651870
391.739703	7441.434302	14.756096	-0.077256	4.649389
391.770133	7433.422872	14.761101	-0.077256	4.646922
392.274185	7425.386145	14.766106	-0.077345	4.644445
391.897756	7417.486634	14.771111	-0.077269	4.642010
391.828361	7409.425249	14.776115	-0.077251	4.639523
392.052053	7401.489299	14.781120	-0.077288	4.637074
391.997495	7393.387973	14.786125	-0.077272	4.634572
392.201386	7385.443249	14.791130	-0.077305	4.632118
391.965758	7377.405398	14.796135	-0.077256	4.629633
391.958989	7369.460372	14.801139	-0.077249	4.627176
391.876418	7361.383563	14.806144	-0.077229	4.624676
391.423408	7353.477264	14.811149	-0.077139	4.622228
392.094868	7345.388370	14.816154	-0.077259	4.619723
392.013396	7337.409211	14.821159	-0.077238	4.617249
392.374453	7329.321463	14.826163	-0.077300	4.614742
392.390971	7321.399915	14.831168	-0.077298	4.612284
392.536276	7313.292185	14.836173	-0.077320	4.609767
392.145410	7305.482987	14.841178	-0.077242	4.607340
391.566459	7297.428651	14.846183	-0.077129	4.604837
391.862869	7289.465056	14.851187	-0.077179	4.602361
391.563910	7281.437713	14.856192	-0.077118	4.599863
391.042500	7273.507998	14.861197	-0.077016	4.597393
391.129966	7265.390780	14.866202	-0.077027	4.594865
391.466288	7257.379052	14.871207	-0.077084	4.592369
391.342148	7249.322642	14.876211	-0.077056	4.589857
391.595696	7241.396932	14.881216	-0.077098	4.587384
391.543146	7233.275964	14.886221	-0.077082	4.584849
391.531218	7225.390150	14.891226	-0.077075	4.582386
391.519775	7217.350777	14.896231	-0.077068	4.579874
391.682552	7209.393713	14.901235	-0.077093	4.577386
391.606486	7201.359495	14.906240	-0.077073	4.574873
391.473094	7193.363977	14.911245	-0.077043	4.572370
391.549111	7185.336722	14.916250	-0.077052	4.569856
391.563506	7177.348121	14.921255	-0.077050	4.567353
391.383871	7169.323367	14.926259	-0.077011	4.564837
391.299753	7161.389030	14.931264	-0.076990	4.562347
391.197475	7153.343841	14.936269	-0.076966	4.559822
391.586237	7145.372196	14.941274	-0.077033	4.557319
391.347385	7137.305099	14.946279	-0.076983	4.554784
391.432510	7129.340422	14.951283	-0.076994	4.552280
391.500252	7121.267125	14.956288	-0.077001	4.549741
390.892536	7113.362336	14.961293	-0.076883	4.547251
390.756528	7105.373056	14.966298	-0.076852	4.544735
390.671589	7097.411611	14.971303	-0.076831	4.542226
390.679524	7089.307298	14.976307	-0.076827	4.539671
390.727265	7081.349684	14.981312	-0.076831	4.537161
390.451374	7073.273756	14.986317	-0.076774	4.534611
390.652986	7065.366159	14.991322	-0.076806	4.532115
390.334670	7057.278026	14.996327	-0.076742	4.529558
390.690285	7049.263230	15.001331	-0.076803	4.527025
390.999386	7041.206865	15.006336	-0.076855	4.524478
390.746502	7033.353749	15.011341	-0.076803	4.521991
391.099621	7025.281152	15.016346	-0.076863	4.519436
390.882660	7017.351812	15.021351	-0.076818	4.516923
390.349365	7009.344637	15.026355	-0.076713	4.514382
390.212343	7001.360600	15.031360	-0.076682	4.511849
390.322339	6993.243715	15.036365	-0.076698	4.509273
389.955818	6985.335210	15.041370	-0.076624	4.506760
389.808304	6977.227457	15.046375	-0.076591	4.504183
390.161284	6969.262012	15.051379	-0.076652	4.501652
390.116924	6961.248630	15.056384	-0.076638	4.499103
389.831229	6953.233841	15.061389	-0.076580	4.496550
390.379074	6945.170598	15.066394	-0.076677	4.493984
390.257145	6937.275651	15.071399	-0.076649	4.491468
389.713114	6929.259247	15.076403	-0.076542	4.488910
390.163655	6921.219464	15.081408	-0.076621	4.486347
390.329753	6913.174054	15.086413	-0.076646	4.483779
390.487394	6905.299428	15.091418	-0.076671	4.481265
390.366050	6897.192585	15.096423	-0.076643	4.478673
390.213313	6889.237322	15.101427	-0.076609	4.476129
389.853348	6881.267023	15.106432	-0.076537	4.473577
390.272084	6873.174696	15.111437	-0.076609	4.470989
390.165227	6865.232590	15.116442	-0.076584	4.468444
390.026538	6857.223445	15.121447	-0.076553	4.465877
390.308049	6849.190562	15.126451	-0.076600	4.463302
390.199502	6841.222348	15.131456	-0.076575	4.460745
390.239738	6833.215734	15.136461	-0.076577	4.458174
390.002474	6825.271305	15.141466	-0.076528	4.455621
389.830495	6817.192661	15.146471	-0.076490	4.453024
389.854445	6809.175977	15.151475	-0.076490	4.450445
390.080678	6801.210268	15.156480	-0.076526	4.447883
389.942522	6793.198563	15.161485	-0.076495	4.445303
389.728719	6785.257681	15.166490	-0.076450	4.442743
389.730746	6777.187291	15.171495	-0.076445	4.440142
389.911993	6769.200004	15.176499	-0.076474	4.437567
389.633165	6761.199720	15.181504	-0.076417	4.434983
389.150303	6753.214381	15.186509	-0.076322	4.432402
389.440704	6745.163874	15.191514	-0.076370	4.429802
389.136338	6737.221763	15.196519	-0.076309	4.427233
388.241861	6729.240540	15.201523	-0.076137	4.424646
388.675110	6721.200699	15.206528	-0.076212	4.422046
388.180858	6713.221286	15.211533	-0.076115	4.419459
388.497545	6705.183177	15.216538	-0.076169	4.416856
388.061377	6697.180581	15.221543	-0.076082	4.414258
388.646209	6689.103678	15.226547	-0.076186	4.411641
389.136948	6681.053264	15.231552	-0.076272	4.409030
388.994538	6673.089348	15.236557	-0.076240	4.406442
389.697765	6665.025940	15.241562	-0.076366	4.403826
389.505347	6657.202866	15.246567	-0.076325	4.401280
389.065081	6649.188695	15.251571	-0.076237	4.398670
389.183325	6641.237664	15.256576	-0.076254	4.396082
389.310491	6633.125369	15.261581	-0.076273	4.393440
389.432516	6625.156839	15.266586	-0.076290	4.390843
389.293899	6617.127375	15.271591	-0.076259	4.388223
389.390223	6609.143938	15.276595	-0.076272	4.385618
389.210361	6601.191857	15.281600	-0.076233	4.383020
388.584118	6593.250871	15.286605	-0.076111	4.380421
388.554971	6585.307253	15.291610	-0.076101	4.377823
388.316998	6577.258260	15.296615	-0.076051	4.375188
388.701450	6569.223005	15.301619	-0.076117	4.372560
388.976477	6561.193814	15.306624	-0.076163	4.369932
388.697155	6553.214600	15.311629	-0.076106	4.367315
388.572768	6545.243589	15.316634	-0.076078	4.364700
388.211139	6537.292117	15.321639	-0.076005	4.362088
388.570192	6529.215581	15.326643	-0.076067	4.359439
388.130059	6521.335465	15.331648	-0.075979	4.356847
388.098607	6513.234579	15.336653	-0.075968	4.354183
388.412540	6505.204848	15.341658	-0.076021	4.351544
388.056945	6497.168627	15.346663	-0.075950	4.348896
387.610475	6489.227677	15.351667	-0.075862	4.346278
387.572433	6481.213068	15.356672	-0.075849	4.343636
388.176247	6473.169379	15.361677	-0.075956	4.340988
387.787657	6465.255981	15.366682	-0.075879	4.338374
387.813636	6457.206235	15.371687	-0.075878	4.335717
388.068293	6449.210723	15.376691	-0.075921	4.333078
388.272621	6441.178720	15.381696	-0.075953	4.330424
388.124322	6433.205466	15.386701	-0.075920	4.327786
388.173435	6425.200222	15.391706	-0.075924	4.325137
388.440346	6417.244420	15.396711	-0.075969	4.322504
388.394270	6409.152370	15.401715	-0.075955	4.319822
388.037516	6401.334876	15.406720	-0.075883	4.317227
388.105778	6393.210416	15.411725	-0.075891	4.314533
388.134568	6385.285689	15.416730	-0.075891	4.311902
387.622751	6377.220000	15.421735	-0.075790	4.309218
387.206782	6369.284761	15.426739	-0.075708	4.306577
387.197793	6361.195658	15.431744	-0.075701	4.303886
386.673566	6353.284625	15.436749	-0.075598	4.301249
387.096039	6345.180150	15.441754	-0.075671	4.298554
387.070990	6337.188097	15.446759	-0.075661	4.295890
386.710604	6329.173546	15.451763	-0.075589	4.293215
386.734241	6321.171500	15.456768	-0.075588	4.290545
386.416998	6313.188421	15.461773	-0.075524	4.287877
386.527986	6305.169700	15.466778	-0.075539	4.285199
386.481215	6297.208878	15.471783	-0.075525	4.282538
386.540111	6289.185699	15.476787	-0.075531	4.279855
386.753955	6281.196752	15.481792	-0.075566	4.277183
386.970635	6273.070985	15.486797	-0.075601	4.274464
386.778301	6265.171511	15.491802	-0.075560	4.271815
386.823649	6257.134315	15.496807	-0.075563	4.269120
386.036235	6249.245290	15.501811	-0.075411	4.266466
386.344309	6241.167910	15.506816	-0.075463	4.263757
386.394579	6233.169049	15.511821	-0.075467	4.261070
386.451823	6225.153661	15.516826	-0.075472	4.258376
386.138804	6217.206267	15.521831	-0.075409	4.255699
386.104428	6209.154623	15.526835	-0.075397	4.252989
386.071570	6201.185926	15.531840	-0.075386	4.250304
385.877712	6193.160477	15.536845	-0.075345	4.247598
386.090788	6185.113966	15.541850	-0.075379	4.244886
386.276426	6177.144572	15.546855	-0.075408	4.242199
386.066565	6169.147983	15.551859	-0.075364	4.239496
386.175545	6161.186417	15.556864	-0.075379	4.236807
386.082159	6153.160490	15.561869	-0.075356	4.234093
385.962059	6145.184874	15.566874	-0.075329	4.231393
386.595399	6137.066147	15.571879	-0.075441	4.228652
386.407333	6129.122266	15.576883	-0.075401	4.225958
386.115771	6121.182238	15.581888	-0.075342	4.223264
385.762890	6113.156444	15.586893	-0.075271	4.220538
386.275156	6105.123620	15.591898	-0.075361	4.217817
386.079079	6097.148246	15.596903	-0.075319	4.215106
385.658234	6089.213921	15.601907	-0.075235	4.212405
385.857694	6081.120341	15.606912	-0.075267	4.209655
385.673915	6073.179498	15.611917	-0.075228	4.206950
385.516546	6065.132977	15.616922	-0.075193	4.204209
384.819036	6057.276590	15.621927	-0.075058	4.201524
385.039923	6049.184015	15.626931	-0.075094	4.198767
385.200132	6041.226795	15.631936	-0.075119	4.196054
384.846418	6033.132217	15.636941	-0.075047	4.193286
384.756184	6025.156513	15.641946	-0.075025	4.190561
385.021406	6017.046878	15.646951	-0.075069	4.187791
385.127861	6009.065709	15.651955	-0.075084	4.185062
385.196662	6001.139346	15.656960	-0.075092	4.182350
385.081653	5993.078766	15.661965	-0.075065	4.179588
385.055658	5985.155193	15.666970	-0.075055	4.176872
384.855400	5977.109209	15.671975	-0.075012	4.174110
384.849462	5969.129003	15.676979	-0.075006	4.171371
384.967542	5961.105072	15.681984	-0.075023	4.168616
384.839100	5953.079851	15.686989	-0.074993	4.165857
385.317938	5945.091545	15.691994	-0.075077	4.163116
385.531548	5937.094395	15.696999	-0.075112	4.160366
385.235319	5929.155566	15.702003	-0.075052	4.157629
385.243364	5921.161980	15.707008	-0.075048	4.154875
385.224129	5913.178330	15.712013	-0.075039	4.152122
384.786011	5905.186630	15.717018	-0.074952	4.149359
384.469273	5897.231156	15.722023	-0.074888	4.146608
384.503263	5889.153188	15.727027	-0.074889	4.143818
384.858219	5881.176852	15.732032	-0.074950	4.141065
384.327944	5873.159921	15.737037	-0.074846	4.138284
384.307709	5865.185026	15.742042	-0.074837	4.135523
384.315420	5857.174759	15.747047	-0.074833	4.132748
384.557695	5849.116716	15.752051	-0.074873	4.129958
384.199211	5841.224965	15.757056	-0.074801	4.127216
384.198803	5833.124169	15.762061	-0.074795	4.124404
384.386425	5825.186863	15.767066	-0.074825	4.121649
384.405234	5817.119570	15.772071	-0.074823	4.118845
384.149304	5809.231038	15.777075	-0.074771	4.116098
384.009754	5801.206073	15.782080	-0.074739	4.113303
383.776777	5793.167061	15.787085	-0.074691	4.110500
383.968898	5785.134490	15.792090	-0.074721	4.107703
383.741588	5777.190445	15.797095	-0.074674	4.104929
383.152823	5769.260253	15.802099	-0.074559	4.102153
383.382467	5761.180840	15.807104	-0.074596	4.099334
383.251868	5753.202891	15.812109	-0.074567	4.096544
383.140708	5745.202868	15.817114	-0.074541	4.093744
383.358843	5737.133245	15.822119	-0.074576	4.090923
382.942873	5729.153333	15.827123	-0.074493	4.088123
382.606929	5721.236289	15.832128	-0.074426	4.085343
382.854831	5713.172189	15.837133	-0.074466	4.082519
382.999491	5705.136591	15.842138	-0.074488	4.079701
382.641451	5697.207716	15.847143	-0.074416	4.076911
382.860865	5689.101836	15.852147	-0.074452	4.074066
382.618269	5681.235998	15.857152	-0.074401	4.071296
382.665134	5673.109587	15.862157	-0.074405	4.068437
382.762961	5665.146200	15.867162	-0.074418	4.065634
382.919344	5657.121978	15.872167	-0.074442	4.062808
382.814320	5649.127904	15.877171	-0.074417	4.059988
382.702137	5641.210498	15.882176	-0.074391	4.057192
382.628958	5633.129866	15.887181	-0.074372	4.054337
382.684076	5625.160593	15.892186	-0.074377	4.051522
382.716692	5617.115764	15.897191	-0.074378	4.048677
383.228496	5609.065013	15.902195	-0.074468	4.045836
383.007694	5601.147549	15.907200	-0.074421	4.043029
383.096281	5593.129361	15.912205	-0.074433	4.040189
382.728718	5585.264019	15.917210	-0.074359	4.037394
382.585213	5577.178705	15.922215	-0.074327	4.034522
382.605331	5569.141887	15.927219	-0.074325	4.031668
382.724252	5561.124699	15.932224	-0.074342	4.028821
382.409654	5553.126824	15.937229	-0.074278	4.025971
382.044400	5545.193201	15.942234	-0.074205	4.023142
382.236164	5537.180034	15.947239	-0.074236	4.020291
382.256181	5529.209332	15.952243	-0.074234	4.017451
382.349487	5521.175227	15.957248	-0.074246	4.014587
382.177637	5513.179321	15.962253	-0.074209	4.011730
382.576777	5505.146678	15.967258	-0.074278	4.008868
382.575957	5497.163772	15.972263	-0.074273	4.006015
381.913452	5489.223961	15.977267	-0.074144	4.003164
382.009481	5481.242737	15.982272	-0.074157	4.000309
381.714147	5473.227460	15.987277	-0.074096	3.997433
381.836741	5465.216360	15.992282	-0.074114	3.994563
381.951986	5457.193924	15.997287	-0.074130	3.991688
382.316588	5449.133894	16.002291	-0.074193	3.988801
382.254376	5441.183639	16.007296	-0.074176	3.985944
381.807015	5433.212708	16.012301	-0.074088	3.983071
382.108157	5425.199889	16.017306	-0.074138	3.980193
381.907100	5417.225171	16.022311	-0.074096	3.977319
381.559235	5409.241014	16.027315	-0.074026	3.974437
381.446587	5401.269358	16.032320	-0.073999	3.971561
381.626357	5393.180029	16.037325	-0.074028	3.968645
381.376801	5385.251940	16.042330	-0.073976	3.965778
381.694335	5377.211509	16.047335	-0.074030	3.962879
381.536270	5369.206751	16.052339	-0.073995	3.959982
380.908226	5361.338557	16.057344	-0.073873	3.957123
380.703804	5353.262699	16.062349	-0.073830	3.954195
381.308932	5345.202617	16.067354	-0.073937	3.951285
380.813321	5337.244780	16.072359	-0.073839	3.948390
380.526151	5329.232456	16.077363	-0.073781	3.945477
380.596098	5321.240488	16.082368	-0.073789	3.942576
380.671624	5313.188835	16.087373	-0.073797	3.939651
380.642249	5305.242948	16.092378	-0.073787	3.936760
380.322289	5297.242561	16.097383	-0.073722	3.933842
380.445098	5289.192611	16.102387	-0.073739	3.930912
380.540586	5281.223673	16.107392	-0.073752	3.928009
379.930585	5273.283107	16.112397	-0.073633	3.925100
380.497479	5265.211420	16.117402	-0.073733	3.922165
380.274687	5257.248831	16.122407	-0.073687	3.919251
380.489773	5249.249378	16.127411	-0.073721	3.916330
380.162369	5241.257429	16.132416	-0.073655	3.913400
380.211870	5233.208837	16.137421	-0.073659	3.910454
380.328412	5225.235087	16.142426	-0.073676	3.907534
380.511551	5217.164097	16.147431	-0.073704	3.904578
380.594206	5209.268703	16.152435	-0.073715	3.901682
380.525614	5201.254792	16.157440	-0.073697	3.898737
380.566441	5193.274126	16.162445	-0.073699	3.895804
380.275512	5185.287896	16.167450	-0.073640	3.892861
380.410323	5177.237010	16.172455	-0.073659	3.889900
380.130915	5169.312425	16.177459	-0.073602	3.886975
379.929517	5161.337985	16.182464	-0.073559	3.884031
379.814858	5153.342039	16.187469	-0.073533	3.881079
380.866039	5145.207089	16.192474	-0.073723	3.878096
380.366695	5137.290338	16.197479	-0.073625	3.875161
380.603251	5129.107353	16.202483	-0.073664	3.872140
380.253692	5121.180323	16.207488	-0.073593	3.869199
380.318117	5113.201579	16.212493	-0.073600	3.866245
380.112412	5105.252620	16.217498	-0.073557	3.863294
380.057569	5097.262560	16.222503	-0.073541	3.860329
379.851734	5089.298201	16.227507	-0.073498	3.857369
379.694206	5081.334771	16.232512	-0.073463	3.854407
379.670422	5073.303553	16.237517	-0.073453	3.851420
380.179568	5065.233647	16.242522	-0.073543	3.848428
379.594989	5057.320132	16.247527	-0.073429	3.845469
379.188900	5049.369126	16.252531	-0.073348	3.842497
379.411090	5041.323493	16.257536	-0.073384	3.839501
378.664282	5033.442584	16.262541	-0.073240	3.836544
379.163437	5025.308011	16.267546	-0.073327	3.833516
379.494424	5017.248800	16.272551	-0.073384	3.830510
379.202452	5009.298381	16.277555	-0.073324	3.827529
379.532816	5001.237483	16.282560	-0.073380	3.824519
378.983767	4993.374870	16.287565	-0.073273	3.821560
379.320111	4985.326932	16.292570	-0.073330	3.818550
379.312360	4977.295763	16.297575	-0.073324	3.815535
379.156989	4969.329644	16.302579	-0.073289	3.812540
379.333107	4961.266092	16.307584	-0.073317	3.809513
379.267737	4953.312197	16.312589	-0.073300	3.806519
378.799254	4945.410521	16.317594	-0.073207	3.803533
378.963448	4937.347673	16.322599	-0.073232	3.800499
378.825764	4929.380743	16.327603	-0.073202	3.797492
378.730851	4921.379540	16.332608	-0.073179	3.794470
378.343933	4913.400164	16.337613	-0.073101	3.791447
378.074058	4905.416834	16.342618	-0.073046	3.788423
378.352799	4897.336895	16.347623	-0.073092	3.785373
378.696304	4889.308805	16.352627	-0.073151	3.782342
379.128243	4881.276583	16.357632	-0.073226	3.779308
378.394774	4873.409539	16.362637	-0.073085	3.776308
378.443883	4865.360447	16.367642	-0.073088	3.773254
378.994694	4857.310277	16.372647	-0.073186	3.770209
378.495454	4849.408660	16.377651	-0.073088	3.767194
377.997363	4841.418368	16.382656	-0.072990	3.764142
377.996435	4833.481233	16.387661	-0.072984	3.761120
378.117481	4825.425643	16.392666	-0.073001	3.758053
378.127047	4817.424583	16.397671	-0.072998	3.755002
378.045784	4809.445632	16.402675	-0.072978	3.751955
377.968262	4801.423130	16.407680	-0.072958	3.748888
378.024037	4793.370929	16.412685	-0.072963	3.745811
377.766559	4785.453144	16.417690	-0.072910	3.742775
377.993321	4777.418560	16.422695	-0.072947	3.739704
377.835753	4769.436533	16.427699	-0.072912	3.736641
378.368622	4761.347956	16.432704	-0.073006	3.733552
377.892199	4753.454322	16.437709	-0.072912	3.730510
378.210398	4745.433406	16.442714	-0.072966	3.727436
377.828285	4737.421018	16.447719	-0.072890	3.724346
377.738761	4729.489490	16.452723	-0.072868	3.721291
378.319235	4721.452312	16.457728	-0.072971	3.718211
377.783268	4713.505038	16.462733	-0.072866	3.715134
377.931135	4705.421390	16.467738	-0.072888	3.712019
377.637486	4697.456257	16.472743	-0.072828	3.708936
377.768742	4689.417872	16.477747	-0.072847	3.705833
377.762884	4681.437293	16.482752	-0.072841	3.702746
376.954707	4673.537331	16.487757	-0.072685	3.699667
377.157794	4665.530388	16.492762	-0.072718	3.696570
377.755019	4657.393227	16.497767	-0.072824	3.693431
377.748985	4649.387963	16.502771	-0.072817	3.690324
377.504404	4641.498031	16.507776	-0.072766	3.687253
377.193172	4633.474010	16.512781	-0.072703	3.684126
377.428963	4625.554390	16.517786	-0.072742	3.681051
377.377315	4617.542335	16.522791	-0.072727	3.677930
377.356006	4609.537432	16.527795	-0.072718	3.674810
377.263188	4601.529060	16.532800	-0.072695	3.671684
376.957913	4593.524626	16.537805	-0.072633	3.668551
377.097061	4585.521985	16.542810	-0.072654	3.665428
377.375477	4577.490111	16.547815	-0.072700	3.662295
376.978434	4569.551851	16.552819	-0.072621	3.659177
376.749523	4561.631118	16.557824	-0.072573	3.656068
376.507998	4553.593938	16.562829	-0.072523	3.652911
376.420145	4545.619050	16.567834	-0.072502	3.649779
376.499756	4537.575704	16.572839	-0.072511	3.646622
376.690325	4529.529877	16.577843	-0.072541	3.643465
376.923706	4521.572794	16.582848	-0.072580	3.640341
376.551120	4513.630548	16.587853	-0.072505	3.637204
376.275675	4505.629030	16.592858	-0.072448	3.634043
376.417781	4497.596914	16.597863	-0.072470	3.630879
376.802505	4489.499060	16.602867	-0.072536	3.627693
376.701600	4481.563021	16.607872	-0.072512	3.624554
376.647639	4473.598178	16.612877	-0.072497	3.621403
376.251384	4465.681530	16.617882	-0.072418	3.618258
376.583416	4457.608238	16.622887	-0.072474	3.615069
376.541003	4449.599757	16.627891	-0.072461	3.611892
376.591348	4441.586888	16.632896	-0.072465	3.608714
376.479193	4433.586617	16.637901	-0.072439	3.605533
376.276250	4425.679374	16.642906	-0.072396	3.602383
376.363918	4417.654335	16.647911	-0.072407	3.599193
376.319268	4409.656282	16.652915	-0.072394	3.596006
376.286057	4401.653543	16.657920	-0.072382	3.592815
375.829734	4393.713419	16.662925	-0.072292	3.589634
375.666158	4385.733869	16.667930	-0.072256	3.586442
375.755744	4377.699770	16.672935	-0.072268	3.583234
375.670506	4369.681161	16.677939	-0.072246	3.580024
375.688755	4361.714286	16.682944	-0.072245	3.576834
375.555700	4353.674728	16.687949	-0.072215	3.573608
375.737392	4345.672571	16.692954	-0.072243	3.570404
375.604732	4337.707373	16.697959	-0.072213	3.567202
374.962185	4329.738907	16.702963	-0.072088	3.563980
375.555698	4321.734183	16.707968	-0.072194	3.560779
375.503865	4313.722503	16.712973	-0.072179	3.557552
375.097349	4305.796177	16.717978	-0.072098	3.554345
374.727580	4297.790058	16.722983	-0.072024	3.551105
375.000669	4289.678177	16.727987	-0.072069	3.547839
374.963725	4281.709365	16.732992	-0.072057	3.544618
374.928358	4273.746154	16.737997	-0.072045	3.541396
374.909120	4265.755820	16.743002	-0.072036	3.538161
374.734981	4257.770122	16.748007	-0.071999	3.534920
374.012380	4249.874252	16.753011	-0.071859	3.531696
374.389926	4241.753818	16.758016	-0.071924	3.528411
373.983432	4233.813839	16.763021	-0.071843	3.525172
373.838378	4225.864051	16.768026	-0.071811	3.521935
374.069041	4217.770408	16.773031	-0.071849	3.518648
374.134929	4209.785209	16.778035	-0.071856	3.515397
374.261960	4201.786504	16.783040	-0.071874	3.512139
374.294157	4193.778929	16.788045	-0.071875	3.508871
374.130645	4185.811041	16.793050	-0.071839	3.505611
374.454349	4177.773974	16.798055	-0.071894	3.502334
374.314664	4169.802355	16.803059	-0.071863	3.499067
374.465089	4161.848716	16.808064	-0.071886	3.495813
374.410677	4153.810678	16.813069	-0.071870	3.492515
374.657887	4145.779749	16.818074	-0.071911	3.489227
374.511592	4137.855370	16.823079	-0.071878	3.485966
374.266746	4129.868986	16.828083	-0.071828	3.482674
374.604414	4121.876787	16.833088	-0.071885	3.479395
374.096147	4113.941981	16.838093	-0.071785	3.476109
374.071770	4105.930422	16.843098	-0.071776	3.472804
374.480671	4097.863445	16.848103	-0.071846	3.469487
374.352287	4089.896705	16.853107	-0.071817	3.466191
374.172450	4081.937268	16.858112	-0.071779	3.462893
374.047185	4073.925273	16.863117	-0.071750	3.459572
374.038567	4065.961949	16.868122	-0.071743	3.456271
373.721298	4057.986401	16.873127	-0.071679	3.452952
373.443410	4049.964331	16.878131	-0.071622	3.449612
373.520051	4042.013324	16.883136	-0.071631	3.446310
373.144499	4034.027720	16.888141	-0.071556	3.442975
373.327276	4026.007585	16.893146	-0.071584	3.439642
372.959627	4018.099186	16.898151	-0.071511	3.436333
372.960153	4010.008669	16.903155	-0.071506	3.432958
373.337291	4001.967212	16.908160	-0.071571	3.429612
373.334529	3993.977846	16.913165	-0.071565	3.426272
373.286673	3986.042557	16.918170	-0.071551	3.422950
372.917662	3978.051798	16.923175	-0.071477	3.419590
372.991638	3970.069032	16.928179	-0.071485	3.416246
372.978311	3962.088771	16.933184	-0.071478	3.412897
372.548789	3954.058666	16.938189	-0.071392	3.409508
372.776839	3946.060472	16.943194	-0.071429	3.406153
372.794009	3938.102039	16.948199	-0.071427	3.402803
373.142107	3930.034417	16.953203	-0.071487	3.399417
372.735334	3922.166288	16.958208	-0.071406	3.396084
372.945525	3914.030881	16.963213	-0.071440	3.392657
372.865535	3906.039948	16.968218	-0.071420	3.389277
372.526237	3898.100677	16.973223	-0.071351	3.385906
371.895703	3890.180531	16.978227	-0.071229	3.382529
372.153854	3882.137495	16.983232	-0.071271	3.379129
372.119244	3874.145385	16.988237	-0.071260	3.375737
371.852806	3866.182879	16.993242	-0.071205	3.372345
372.031604	3858.101793	16.998247	-0.071233	3.368916
372.157466	3850.107513	17.003251	-0.071251	3.365518
371.661932	3842.232561	17.008256	-0.071154	3.362145
371.772824	3834.196418	17.013261	-0.071169	3.358722
371.944414	3826.198920	17.018266	-0.071196	3.355314
371.547892	3818.268825	17.023271	-0.071117	3.351911
371.816351	3810.184900	17.028275	-0.071161	3.348463
371.906088	3802.212379	17.033280	-0.071173	3.345052
371.817138	3794.244082	17.038285	-0.071151	3.341633
372.134583	3786.206551	17.043290	-0.071205	3.338197
371.567483	3778.299230	17.048295	-0.071094	3.334779
371.694741	3770.257986	17.053299	-0.071113	3.331326
371.678061	3762.277723	17.058304	-0.071104	3.327891
371.433809	3754.278965	17.063309	-0.071053	3.324435
371.563182	3746.336954	17.068314	-0.071072	3.321014
371.298142	3738.379184	17.073319	-0.071018	3.317568
371.548909	3730.275150	17.078323	-0.071059	3.314075
371.852854	3722.299520	17.083328	-0.071110	3.310637
371.193780	3714.375033	17.088333	-0.070983	3.307179
370.968010	3706.365255	17.093338	-0.070935	3.303697
371.128903	3698.369952	17.098343	-0.070960	3.300233
371.587665	3690.301323	17.103347	-0.071040	3.296746
371.622812	3682.311872	17.108352	-0.071041	3.293272
371.479524	3674.329203	17.113357	-0.071009	3.289791
371.435439	3666.386792	17.118362	-0.070996	3.286327
370.863691	3658.497558	17.123367	-0.070884	3.282862
370.756686	3650.470670	17.128371	-0.070859	3.279352
370.952298	3642.495945	17.133376	-0.070890	3.275872
371.469477	3634.391594	17.138381	-0.070981	3.272346
370.814039	3626.490970	17.143386	-0.070854	3.268857
370.725194	3618.492571	17.148391	-0.070832	3.265345
370.433755	3610.562128	17.153395	-0.070773	3.261851
370.853535	3602.501082	17.158400	-0.070846	3.258324
370.423632	3594.534831	17.163405	-0.070760	3.254800
370.948055	3586.441560	17.168410	-0.070853	3.251256
371.119699	3578.473356	17.173415	-0.070880	3.247749
370.421797	3570.571891	17.178419	-0.070744	3.244232
370.507295	3562.612791	17.183424	-0.070755	3.240717
370.617638	3554.591546	17.188429	-0.070770	3.237172
370.706240	3546.583905	17.193434	-0.070782	3.233629
370.951765	3538.532875	17.198439	-0.070822	3.230069
370.900324	3530.521547	17.203443	-0.070807	3.226510
370.846288	3522.593051	17.208448	-0.070792	3.222984
370.756719	3514.591783	17.213453	-0.070770	3.219420
370.669863	3506.639094	17.218458	-0.070749	3.215874
370.529638	3498.664632	17.223463	-0.070717	3.212313
369.908190	3490.701105	17.228467	-0.070596	3.208731
369.749168	3482.722684	17.233472	-0.070561	3.205158
369.891034	3474.676906	17.238477	-0.070583	3.201565
369.646662	3466.749730	17.243482	-0.070532	3.198003
369.396654	3458.763861	17.248487	-0.070480	3.194412
369.412577	3450.772514	17.253491	-0.070478	3.190825
369.543743	3442.715113	17.258496	-0.070497	3.187209
369.527379	3434.726882	17.263501	-0.070489	3.183614
369.673404	3426.742976	17.268506	-0.070511	3.180024
370.359971	3418.664144	17.273511	-0.070633	3.176411
370.690837	3410.601941	17.278515	-0.070689	3.172786
370.571960	3402.695649	17.283520	-0.070662	3.169207
369.903524	3394.841182	17.288525	-0.070532	3.165623
370.091795	3386.830532	17.293530	-0.070562	3.162003
370.299457	3378.774083	17.298535	-0.070596	3.158358
370.234941	3370.823075	17.303539	-0.070578	3.154745
370.086211	3362.875802	17.308544	-0.070546	3.151126
369.932110	3354.853941	17.313549	-0.070512	3.147468
369.711307	3346.891927	17.318554	-0.070465	3.143830
369.474061	3338.964816	17.323559	-0.070416	3.140203
369.175029	3330.980717	17.328563	-0.070355	3.136543
369.005127	3323.004809	17.333568	-0.070318	3.132889
369.069927	3314.926229	17.338573	-0.070325	3.129194
369.774296	3306.850977	17.343578	-0.070451	3.125525
369.266161	3298.975879	17.348583	-0.070351	3.121888
369.256105	3290.982033	17.353587	-0.070344	3.118215
369.200093	3283.034126	17.358592	-0.070328	3.114557
368.741939	3275.070444	17.363597	-0.070238	3.110869
368.647070	3267.071587	17.368602	-0.070215	3.107177
368.723635	3259.052753	17.373607	-0.070224	3.103479
368.928299	3250.999380	17.378611	-0.070256	3.099767
368.797654	3243.109688	17.383616	-0.070227	3.096111
368.847377	3235.064844	17.388621	-0.070231	3.092386
368.185666	3227.167549	17.393626	-0.070102	3.088692
368.186623	3219.163214	17.398631	-0.070097	3.084976
368.371875	3211.139576	17.403635	-0.070127	3.081254
368.411300	3203.155258	17.408640	-0.070129	3.077540
368.406017	3195.144989	17.413645	-0.070122	3.073806
368.231167	3187.137857	17.418650	-0.070085	3.070062
368.130090	3179.176382	17.423655	-0.070061	3.066338
368.230619	3171.144412	17.428659	-0.070074	3.062586
367.805875	3163.268610	17.433664	-0.069990	3.058877
367.943366	3155.237738	17.438669	-0.070010	3.055118
367.969684	3147.248183	17.443674	-0.070010	3.051368
367.983423	3139.252490	17.448679	-0.070007	3.047611
367.737348	3131.287811	17.453683	-0.069956	3.043850
367.769487	3123.334462	17.458688	-0.069957	3.040104
367.381364	3115.392616	17.463693	-0.069879	3.036338
367.532931	3107.344722	17.468698	-0.069902	3.032544
367.450965	3099.364370	17.473703	-0.069882	3.028765
367.344782	3091.357041	17.478707	-0.069857	3.024968
367.248277	3083.421314	17.483712	-0.069834	3.021200
367.412033	3075.349062	17.488717	-0.069859	3.017376
367.267902	3067.397687	17.493722	-0.069827	3.013589
367.014007	3059.444435	17.498727	-0.069774	3.009791
366.921854	3051.455350	17.503731	-0.069752	3.005979
367.788079	3043.349507	17.508736	-0.069908	3.002155
367.557649	3035.450901	17.513741	-0.069860	2.998370
367.070130	3027.569007	17.518746	-0.069764	2.994574
367.535497	3019.484566	17.523751	-0.069845	2.990726
367.698390	3011.449250	17.528755	-0.069870	2.986881
367.520077	3003.525845	17.533760	-0.069832	2.983066
367.349664	2995.576129	17.538765	-0.069795	2.979235
367.628484	2987.540962	17.543770	-0.069841	2.975381
367.963887	2979.522242	17.548775	-0.069899	2.971533
367.397457	2971.610724	17.553779	-0.069788	2.967684
367.072332	2963.693925	17.558784	-0.069722	2.963841
366.899717	2955.722002	17.563789	-0.069685	2.959974
366.806599	2947.746787	17.568794	-0.069662	2.956104
366.983731	2939.707589	17.573799	-0.069690	2.952212
366.627712	2931.755115	17.578803	-0.069618	2.948329
366.483591	2923.778577	17.583808	-0.069586	2.944441
366.829266	2915.744233	17.588813	-0.069645	2.940545
366.710384	2907.779681	17.593818	-0.069618	2.936654
366.277165	2899.885240	17.598823	-0.069532	2.932774
366.385670	2891.819944	17.603827	-0.069547	2.928835
366.593654	2883.835998	17.608832	-0.069581	2.924936
366.087042	2875.922525	17.613837	-0.069481	2.921028
365.884204	2867.984993	17.618842	-0.069438	2.917119
366.327699	2859.877360	17.623847	-0.069515	2.913156
366.188239	2851.841523	17.628851	-0.069484	2.909191
366.387912	2843.851714	17.633856	-0.069516	2.905263
366.014514	2835.924528	17.638861	-0.069441	2.901328
365.954986	2827.955554	17.643866	-0.069425	2.897385
366.100561	2819.935434	17.648871	-0.069447	2.893422
365.727567	2812.012689	17.653875	-0.069372	2.889473
366.283901	2803.963911	17.658880	-0.069470	2.885508
366.047855	2796.023210	17.663885	-0.069421	2.881547
365.881628	2788.075033	17.668890	-0.069385	2.877581
366.115969	2780.053251	17.673895	-0.069423	2.873595
365.745562	2772.124616	17.678899	-0.069349	2.869616
365.658764	2764.147590	17.683904	-0.069328	2.865623
365.590079	2756.160353	17.688909	-0.069310	2.861621
365.620096	2748.191779	17.693914	-0.069310	2.857628
365.608258	2740.198075	17.698919	-0.069303	2.853614
365.607992	2732.183896	17.703923	-0.069297	2.849585
365.797624	2724.211409	17.708928	-0.069328	2.845583
365.397217	2716.283529	17.713933	-0.069248	2.841563
365.347674	2708.313886	17.718938	-0.069233	2.837536
365.398510	2700.355163	17.723943	-0.069238	2.833516
365.065148	2692.396443	17.728947	-0.069170	2.829467
365.156708	2684.359730	17.733952	-0.069182	2.825397
364.982398	2676.385504	17.738957	-0.069144	2.821338
365.681147	2668.291857	17.743962	-0.069269	2.817263
365.557399	2660.385032	17.748967	-0.069241	2.813230
364.978758	2652.459179	17.753971	-0.069128	2.809154
365.164244	2644.466143	17.758976	-0.069157	2.805083
365.233033	2636.475619	17.763981	-0.069165	2.801000
365.087397	2628.535102	17.768986	-0.069132	2.796924
365.121538	2620.563352	17.773991	-0.069134	2.792837
364.779285	2612.592616	17.778995	-0.069065	2.788722
365.074707	2604.544577	17.784000	-0.069114	2.784599
364.658071	2596.657846	17.789005	-0.069032	2.780511
364.783372	2588.644278	17.794010	-0.069050	2.776384
364.858132	2580.646693	17.799015	-0.069058	2.772255
364.780793	2572.646964	17.804019	-0.069039	2.768111
364.771357	2564.685548	17.809024	-0.069032	2.763984
364.524080	2556.772578	17.814029	-0.068980	2.759861
364.210850	2548.855381	17.819034	-0.068917	2.755726
364.338549	2540.785258	17.824039	-0.068935	2.751532
363.986916	2532.814865	17.829043	-0.068865	2.747354
364.496099	2524.749505	17.834048	-0.068954	2.743174
364.633874	2516.779816	17.839053	-0.068975	2.739014
364.561858	2508.846026	17.844058	-0.068956	2.734854
364.718874	2500.850559	17.849063	-0.068980	2.730669
364.082401	2492.973046	17.854067	-0.068856	2.726490
363.971631	2485.018779	17.859072	-0.068830	2.722297
364.328040	2476.956730	17.864077	-0.068892	2.718070
363.883661	2469.047187	17.869082	-0.068804	2.713867
363.402150	2461.147549	17.874087	-0.068709	2.709660
363.219714	2453.144788	17.879091	-0.068670	2.705410
363.031217	2445.211903	17.884096	-0.068629	2.701191
362.882583	2437.192137	17.889101	-0.068596	2.696921
362.990995	2429.168608	17.894106	-0.068611	2.692660
363.560184	2421.092322	17.899111	-0.068712	2.688393
363.730185	2413.069543	17.904115	-0.068738	2.684122
363.768835	2405.186915	17.909120	-0.068740	2.679911
363.872932	2397.206111	17.914125	-0.068754	2.675644
363.820334	2389.248420	17.919130	-0.068739	2.671373
363.524069	2381.326956	17.924135	-0.068679	2.667099
363.591484	2373.309938	17.929139	-0.068686	2.662790
363.529573	2365.363433	17.934144	-0.068670	2.658504
363.593129	2357.370981	17.939149	-0.068676	2.654195
363.215557	2349.460873	17.944154	-0.068601	2.649893
363.751569	2341.387614	17.949159	-0.068695	2.645557
363.265470	2333.518996	17.954163	-0.068599	2.641257
363.037859	2325.586085	17.959168	-0.068552	2.636932
363.465788	2317.516754	17.964173	-0.068626	2.632570
363.115566	2309.599606	17.969178	-0.068556	2.628230
363.071805	2301.624734	17.974183	-0.068542	2.623873
363.565800	2293.564714	17.979187	-0.068629	2.619499
363.086362	2285.724258	17.984192	-0.068535	2.615171
363.180425	2277.683497	17.989197	-0.068547	2.610766
363.079764	2269.745053	17.994202	-0.068523	2.606396
362.371818	2261.906076	17.999207	-0.068386	2.602031
362.134174	2253.935606	18.004211	-0.068337	2.597619
361.649164	2246.010226	18.009216	-0.068241	2.593207
361.608123	2237.879486	18.014221	-0.068228	2.588704
361.963152	2229.792537	18.019226	-0.068289	2.584246
362.199940	2221.842405	18.024231	-0.068328	2.579848
361.821290	2213.933694	18.029235	-0.068252	2.575422
361.686291	2205.993071	18.034240	-0.068222	2.570988
361.816903	2197.959006	18.039245	-0.068241	2.566513
361.835808	2190.014163	18.044250	-0.068239	2.562072
362.366819	2181.984713	18.049255	-0.068333	2.557612
362.268990	2174.023311	18.054259	-0.068309	2.553138
362.350182	2166.089396	18.059264	-0.068319	2.548684
361.889666	2158.156897	18.064269	-0.068228	2.544184
361.954817	2150.225261	18.069274	-0.068235	2.539715
362.156011	2142.212800	18.074279	-0.068267	2.535202
362.034078	2134.251602	18.079283	-0.068239	2.530687
362.333484	2126.263096	18.084288	-0.068290	2.526178
362.667880	2118.240225	18.089293	-0.068347	2.521645
362.248872	2110.394883	18.094298	-0.068264	2.517149
362.286244	2102.413434	18.099303	-0.068265	2.512601
361.976748	2094.469753	18.104307	-0.068203	2.508041
361.796793	2086.521725	18.109312	-0.068164	2.503480
361.824802	2078.550395	18.114317	-0.068164	2.498912
361.765050	2070.578420	18.119322	-0.068147	2.494329
361.803000	2062.596473	18.124327	-0.068149	2.489739
362.060582	2054.566201	18.129331	-0.068192	2.485130
361.998751	2046.656663	18.134336	-0.068175	2.480557
361.862692	2038.704336	18.139341	-0.068145	2.475946
362.092293	2030.711992	18.144346	-0.068182	2.471331
362.117856	2022.766037	18.149351	-0.068182	2.466718
361.865536	2014.841687	18.154355	-0.068130	2.462088
361.390667	2006.968106	18.159360	-0.068036	2.457462
361.404430	1998.965400	18.164365	-0.068033	2.452789
361.507286	1990.957372	18.169370	-0.068047	2.448111
361.393838	1983.027220	18.174375	-0.068021	2.443453
361.486348	1975.040650	18.179379	-0.068033	2.438769
361.486941	1967.088168	18.184384	-0.068028	2.434089
361.241157	1959.107779	18.189389	-0.067977	2.429364
361.337270	1951.110013	18.194394	-0.067989	2.424646
361.345600	1943.192646	18.199399	-0.067986	2.419960
360.980338	1935.268639	18.204403	-0.067912	2.415231
360.677333	1927.349176	18.209408	-0.067851	2.410501
360.962473	1919.304724	18.214413	-0.067899	2.405733
360.952591	1911.358400	18.219418	-0.067892	2.400991
361.119225	1903.384533	18.224423	-0.067917	2.396238
360.792855	1895.471759	18.229427	-0.067851	2.391472
360.921734	1887.491126	18.234432	-0.067870	2.386692
360.780643	1879.547192	18.239437	-0.067839	2.381903
360.659453	1871.590755	18.244442	-0.067811	2.377099
360.649493	1863.644229	18.249447	-0.067804	2.372299
360.306926	1855.725527	18.254451	-0.067735	2.367480
360.325190	1847.761683	18.259456	-0.067733	2.362653
360.498905	1839.763230	18.264461	-0.067760	2.357808
359.950517	1831.906597	18.269466	-0.067653	2.352979
359.652447	1823.969509	18.274471	-0.067592	2.348112
359.620219	1815.977903	18.279475	-0.067581	2.343224
359.664299	1808.003518	18.284480	-0.067584	2.338342
359.304711	1800.082606	18.289485	-0.067512	2.333450
359.372666	1792.083289	18.294490	-0.067519	2.328534
359.543449	1784.091776	18.299495	-0.067546	2.323622
359.763180	1776.089875	18.304499	-0.067581	2.318697
359.855478	1768.164134	18.309504	-0.067593	2.313798
359.269778	1760.294097	18.314509	-0.067479	2.308865
359.093563	1752.355003	18.319514	-0.067441	2.303914
359.249678	1744.384980	18.324519	-0.067465	2.298961
359.258067	1736.368271	18.329523	-0.067461	2.293956
359.231079	1728.436475	18.334528	-0.067451	2.288989
359.585227	1720.414147	18.339533	-0.067512	2.283989
359.325037	1712.537779	18.344538	-0.067458	2.279015
359.813627	1704.510133	18.349543	-0.067544	2.274001
359.240326	1696.622877	18.354547	-0.067432	2.268972
358.909315	1688.718506	18.359552	-0.067365	2.263941
358.906525	1680.751953	18.364557	-0.067359	2.258889
358.561096	1672.865306	18.369562	-0.067290	2.253846
358.352245	1664.939245	18.374567	-0.067246	2.248778
358.418344	1656.916467	18.379571	-0.067253	2.243662
358.205105	1649.038832	18.384576	-0.067208	2.238602
358.130945	1641.074030	18.389581	-0.067189	2.233487
358.427898	1633.045231	18.394586	-0.067239	2.228353
358.503125	1625.086754	18.399591	-0.067247	2.223232
358.398978	1617.163877	18.404595	-0.067223	2.218106
358.307843	1609.235856	18.409600	-0.067201	2.212966
358.149562	1601.292783	18.414605	-0.067166	2.207798
357.920828	1593.381261	18.419610	-0.067118	2.202632
358.020622	1585.432050	18.424615	-0.067132	2.197459
357.907750	1577.472012	18.429619	-0.067105	2.192248
358.148674	1569.478039	18.434624	-0.067145	2.187034
358.078670	1561.560983	18.439629	-0.067127	2.181830
358.061703	1553.602929	18.444634	-0.067118	2.176592
358.278700	1545.633460	18.449639	-0.067154	2.171355
357.830153	1537.754616	18.454643	-0.067065	2.166102
358.052785	1529.799811	18.459648	-0.067101	2.160850
358.276488	1521.808170	18.464653	-0.067137	2.155561
358.141452	1513.908052	18.469658	-0.067107	2.150286
358.135111	1505.982989	18.474663	-0.067101	2.144993
357.441612	1498.163329	18.479667	-0.066966	2.139691
357.393755	1490.220779	18.484672	-0.066952	2.134357
357.813732	1482.170571	18.489677	-0.067025	2.128981
357.658347	1474.253550	18.494682	-0.066991	2.123626
357.546748	1466.363863	18.499687	-0.066965	2.118280
357.422607	1458.419849	18.504691	-0.066937	2.112883
357.533048	1450.430290	18.509696	-0.066952	2.107464
357.346522	1442.510495	18.514701	-0.066912	2.102049
357.204357	1434.596331	18.519706	-0.066881	2.096628
357.293256	1426.653814	18.524711	-0.066892	2.091197
357.402587	1418.666886	18.529715	-0.066907	2.085723
357.015269	1410.839239	18.534720	-0.066830	2.080295
357.030125	1402.906188	18.539725	-0.066827	2.074820
356.643706	1395.008879	18.544730	-0.066750	2.069314
356.514704	1387.083665	18.549735	-0.066721	2.063801
356.305155	1379.162630	18.554739	-0.066677	2.058268
356.320375	1371.215026	18.559744	-0.066674	2.052724
356.104537	1363.301922	18.564749	-0.066629	2.047165
355.960147	1355.379481	18.569754	-0.066597	2.041592
356.092230	1347.434414	18.574759	-0.066616	2.036017
356.458301	1339.396187	18.579763	-0.066679	2.030385
356.293019	1331.499775	18.584768	-0.066643	2.024782
356.150371	1323.611424	18.589773	-0.066611	2.019172
355.936974	1315.704299	18.594778	-0.066566	2.013525
356.412588	1307.693774	18.599783	-0.066650	2.007861
355.774351	1299.886137	18.604787	-0.066526	2.002208
356.064336	1291.939556	18.609792	-0.066575	1.996539
355.323465	1284.113959	18.614797	-0.066432	1.990829
355.374363	1276.130085	18.619802	-0.066436	1.985075
355.491168	1268.201016	18.624807	-0.066452	1.979350
355.532771	1260.245875	18.629811	-0.066455	1.973582
355.713930	1252.306077	18.634816	-0.066483	1.967823
355.582290	1244.408736	18.639821	-0.066454	1.962044
355.542894	1236.504061	18.644826	-0.066441	1.956252
355.301129	1228.625646	18.649831	-0.066391	1.950441
355.201759	1220.692501	18.654835	-0.066367	1.944587
355.762240	1212.671527	18.659840	-0.066466	1.938725
355.910917	1204.723254	18.664845	-0.066489	1.932852
355.366952	1196.912736	18.669850	-0.066382	1.926986
355.614888	1188.959064	18.674855	-0.066423	1.921085
355.154548	1181.125914	18.679859	-0.066332	1.915176
355.630452	1173.130095	18.684864	-0.066416	1.909232
355.805826	1165.181415	18.689869	-0.066443	1.903272
355.041656	1157.440689	18.694874	-0.066296	1.897341
354.780485	1149.567454	18.699879	-0.066242	1.891350
354.891467	1141.580511	18.704883	-0.066257	1.885296
354.563287	1133.750797	18.709888	-0.066191	1.879291
354.997464	1125.760244	18.714893	-0.066267	1.873234
355.346876	1117.758721	18.719898	-0.066327	1.867138
354.964249	1109.960638	18.724903	-0.066250	1.861093
354.600237	1102.091257	18.729907	-0.066177	1.854975
354.805395	1094.150980	18.734912	-0.066210	1.848849
354.606655	1086.262854	18.739917	-0.066168	1.842695
354.307714	1078.425050	18.744922	-0.066107	1.836548
354.727688	1070.435673	18.749927	-0.066180	1.830349
354.331535	1062.587295	18.754931	-0.066101	1.824140
354.598899	1054.658984	18.759936	-0.066146	1.817928
354.381674	1046.797825	18.764941	-0.066100	1.811688
354.203082	1038.909383	18.769946	-0.066062	1.805409
354.272332	1031.026474	18.774951	-0.066070	1.799144
354.227489	1023.106116	18.779955	-0.066056	1.792813
354.409736	1015.155064	18.784960	-0.066085	1.786463
354.854476	1007.185743	18.789965	-0.066162	1.780109
354.718733	999.337860	18.794970	-0.066132	1.773757
354.336808	991.541231	18.799975	-0.066056	1.767392
354.052437	983.694884	18.804979	-0.065998	1.760976
354.543566	975.735123	18.809984	-0.066084	1.754544
354.492428	967.861833	18.814989	-0.066069	1.748088
354.177130	960.034252	18.819994	-0.066005	1.741613
353.999583	952.198905	18.824999	-0.065967	1.735125
353.865902	944.300867	18.830003	-0.065937	1.728566
354.326575	936.352568	18.835008	-0.066017	1.722018
353.836778	928.574929	18.840013	-0.065921	1.715462
353.942244	920.666878	18.845018	-0.065936	1.708851
353.609901	912.836068	18.850023	-0.065869	1.702221
353.875093	904.884817	18.855027	-0.065913	1.695543
354.110144	896.981840	18.860032	-0.065951	1.688875
354.005410	889.136959	18.865037	-0.065927	1.682185
353.739798	881.327737	18.870042	-0.065872	1.675476
354.021839	873.412781	18.875047	-0.065919	1.668725
353.587637	865.611901	18.880051	-0.065833	1.661946
353.065596	857.869843	18.885056	-0.065731	1.655178
353.441546	849.898388	18.890061	-0.065796	1.648308
353.489041	842.026308	18.895066	-0.065800	1.641449
353.408717	834.205684	18.900071	-0.065779	1.634589
353.130801	826.341154	18.905075	-0.065723	1.627634
353.523674	818.400072	18.910080	-0.065791	1.620676
353.145319	810.616430	18.915085	-0.065715	1.613718
353.056693	802.765216	18.920090	-0.065693	1.606711
353.148002	794.904867	18.925095	-0.065705	1.599691
353.598708	786.975011	18.930099	-0.065784	1.592629
353.341052	779.190403	18.935104	-0.065731	1.585565
352.709225	771.482575	18.940109	-0.065608	1.578483
352.660179	763.618084	18.945114	-0.065594	1.571313
353.098863	755.694680	18.950119	-0.065670	1.564127
352.964585	747.892349	18.955123	-0.065640	1.556935
352.927945	740.068303	18.960128	-0.065628	1.549704
352.717783	732.262596	18.965133	-0.065584	1.542430
352.956803	724.378545	18.970138	-0.065623	1.535117
352.768616	716.588961	18.975143	-0.065583	1.527791
352.355162	708.833382	18.980147	-0.065501	1.520428
352.303601	701.028544	18.985152	-0.065486	1.513039
352.059939	693.220614	18.990157	-0.065436	1.505580
352.108629	685.388583	18.995162	-0.065440	1.498106
352.055058	677.566648	19.000167	-0.065425	1.490589
351.860884	669.766362	19.005171	-0.065383	1.483032
352.331972	661.873639	19.010176	-0.065466	1.475453
352.051459	654.092725	19.015181	-0.065408	1.467823
351.969945	646.290370	19.020186	-0.065388	1.460164
351.566469	638.573284	19.025191	-0.065308	1.452497
351.521747	630.745421	19.030195	-0.065295	1.444738
351.800817	622.908440	19.035200	-0.065341	1.436981
351.999997	615.066950	19.040205	-0.065373	1.429164
352.040915	607.270049	19.045210	-0.065376	1.421323
352.356683	599.457087	19.050215	-0.065429	1.413469
352.045613	591.731183	19.055219	-0.065366	1.405553
351.765465	584.040452	19.060224	-0.065309	1.397634
351.855040	576.241366	19.065229	-0.065321	1.389621
351.967933	568.434576	19.070234	-0.065337	1.381557
352.094168	560.663081	19.075239	-0.065355	1.373486
352.051116	552.897301	19.080243	-0.065342	1.365343
351.990009	545.185064	19.085248	-0.065326	1.357205
351.717977	537.480892	19.090253	-0.065270	1.348989
351.780011	529.713785	19.095258	-0.065276	1.340714
351.944821	521.954045	19.100263	-0.065302	1.332415
351.600152	514.254385	19.105267	-0.065233	1.324036
351.387431	506.573411	19.110272	-0.065188	1.315649
351.463176	498.721115	19.115277	-0.065197	1.307072
351.049842	491.058614	19.120282	-0.065115	1.298558
350.954861	483.346292	19.125287	-0.065092	1.289992
350.963639	475.607503	19.130291	-0.065089	1.281358
350.948235	467.914169	19.135296	-0.065081	1.272712
350.341762	460.297839	19.140301	-0.064963	1.263981
350.507020	452.552317	19.145306	-0.064989	1.255191
350.256804	444.895117	19.150311	-0.064937	1.246360
350.052612	437.232404	19.155315	-0.064894	1.237468
350.018970	429.540125	19.160320	-0.064883	1.228510
350.227563	421.801383	19.165325	-0.064916	1.219481
350.399774	414.082656	19.170330	-0.064943	1.210401
349.942926	406.502223	19.175335	-0.064853	1.201290
349.515077	398.914705	19.180339	-0.064769	1.192106
349.467751	391.254776	19.185344	-0.064755	1.182841
349.330817	383.612490	19.190349	-0.064724	1.173506
348.659315	376.079768	19.195354	-0.064594	1.164119
348.816323	368.408666	19.200359	-0.064618	1.154659
348.187495	360.847089	19.205363	-0.064496	1.145090
348.421928	353.150579	19.210368	-0.064535	1.135456
348.780758	345.444757	19.215373	-0.064597	1.125756
348.835981	337.834703	19.220378	-0.064602	1.116027
348.036984	330.403387	19.225383	-0.064448	1.106254
347.285304	322.933807	19.230387	-0.064303	1.096354
347.775045	315.235997	19.235392	-0.064390	1.086345
347.716666	307.672545	19.240397	-0.064374	1.076296
347.412099	300.147026	19.245402	-0.064312	1.066145
347.522871	292.564557	19.250407	-0.064328	1.055918
346.883076	285.119722	19.255411	-0.064204	1.045601
346.317514	277.686208	19.260416	-0.064094	1.035214
345.237995	270.334624	19.265421	-0.063888	1.024711
344.391268	262.947088	19.270426	-0.063725	1.014105
343.469766	255.576220	19.275431	-0.063549	1.003393
343.317511	248.052230	19.280435	-0.063515	0.992536
343.324416	240.511839	19.285440	-0.063512	0.981576
342.990623	233.072989	19.290445	-0.063445	0.970554
342.281992	225.721956	19.295450	-0.063308	0.959438
342.144357	218.279889	19.300455	-0.063277	0.948206
342.040324	210.848273	19.305459	-0.063253	0.936864
341.037815	203.612593	19.310464	-0.063062	0.925442
340.476949	196.304455	19.315469	-0.062953	0.913885
340.113578	188.955546	19.320474	-0.062880	0.902169
339.034614	181.781976	19.325479	-0.062674	0.890380
338.072745	174.581989	19.330483	-0.062491	0.878421
337.886527	167.255492	19.335488	-0.062451	0.866315
336.924480	160.113762	19.340493	-0.062267	0.854116
336.742333	152.821600	19.345498	-0.062229	0.841719
336.742499	145.537595	19.350503	-0.062224	0.829206
336.208232	138.361873	19.355507	-0.062120	0.816526
336.173907	131.141589	19.360512	-0.062109	0.803724
335.529659	124.078372	19.365517	-0.061984	0.790803
334.743177	117.060963	19.370522	-0.061833	0.777705
334.380157	110.001027	19.375527	-0.061761	0.764444
333.781309	103.005562	19.380531	-0.061645	0.750991
333.477297	95.995320	19.385536	-0.061583	0.737366
332.910834	89.073791	19.390541	-0.061473	0.723567
332.524396	82.154854	19.395546	-0.061397	0.709570
332.055645	75.474997	19.400551	-0.061305	0.695754