Mon Apr 19 09:21:11 2021

Number of Points = 3642
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.836146	-0.316568	0.000000	-0.000319	0.307070

2.961667	-0.344151	0.005005	-0.000342	0.307047
3.264387	-0.442629	0.010010	-0.000398	0.306842
2.798628	-0.373939	0.015014	-0.000311	0.306766
2.057469	-0.238659	0.020019	-0.000173	0.306769
1.725321	-0.176893	0.025024	-0.000112	0.306775
1.551906	-0.146469	0.030029	-0.000079	0.306769
1.953939	-0.219201	0.035034	-0.000154	0.306770
2.029936	-0.232982	0.040038	-0.000168	0.306770
2.434807	-0.310255	0.045043	-0.000243	0.306752
2.870981	-0.421633	0.050048	-0.000324	0.306600
2.992085	-0.482197	0.055053	-0.000347	0.306418
2.471018	-0.382502	0.060058	-0.000250	0.306441
2.696431	-0.424171	0.065062	-0.000291	0.306437
2.611971	-0.409954	0.070067	-0.000276	0.306432
2.843682	-0.501588	0.075072	-0.000319	0.306197
2.883947	-0.527344	0.080077	-0.000326	0.306110
2.500620	-0.456186	0.085082	-0.000255	0.306116
1.783087	-0.321242	0.090086	-0.000121	0.306138
1.391431	-0.262090	0.095091	-0.000048	0.306080
2.104994	-0.450806	0.100096	-0.000181	0.305801
2.156787	-0.459533	0.105101	-0.000190	0.305804
2.371288	-0.499343	0.110106	-0.000230	0.305799
2.935319	-0.613700	0.115110	-0.000335	0.305743
3.228085	-0.712782	0.120115	-0.000389	0.305525
3.502612	-0.761673	0.125120	-0.000440	0.305529
3.332518	-0.753655	0.130125	-0.000409	0.305421
3.540114	-0.841729	0.135130	-0.000447	0.305181
3.426943	-0.820803	0.140134	-0.000426	0.305183
2.842868	-0.759957	0.145139	-0.000317	0.304968
3.028685	-0.815628	0.150144	-0.000352	0.304863
2.395878	-0.699761	0.155149	-0.000234	0.304867
2.374076	-0.756283	0.160154	-0.000230	0.304579
2.296629	-0.749217	0.165158	-0.000215	0.304546
2.542041	-0.799340	0.170163	-0.000261	0.304519
2.715315	-0.884840	0.175168	-0.000293	0.304262
2.701955	-0.883249	0.180173	-0.000290	0.304257
3.059092	-0.988284	0.185178	-0.000357	0.304066
3.165433	-1.037433	0.190182	-0.000376	0.303924
2.992876	-1.027498	0.195187	-0.000344	0.303821
2.791056	-1.032673	0.200192	-0.000306	0.303622
2.860778	-1.049748	0.205197	-0.000319	0.303600
2.283955	-1.006228	0.210202	-0.000212	0.303308
2.219372	-0.993801	0.215206	-0.000200	0.303310
1.689332	-0.940805	0.220211	-0.000101	0.303103
2.223056	-1.058257	0.225216	-0.000200	0.303005
2.011696	-1.045394	0.230221	-0.000161	0.302883
2.522550	-1.187309	0.235226	-0.000256	0.302648
2.545054	-1.203952	0.240230	-0.000260	0.302587
2.723075	-1.289088	0.245235	-0.000293	0.302334
2.674461	-1.295554	0.250240	-0.000284	0.302261
3.003846	-1.406087	0.255245	-0.000345	0.302018
2.517047	-1.338290	0.260250	-0.000254	0.301918
2.315133	-1.333348	0.265254	-0.000216	0.301766
2.118114	-1.329160	0.270259	-0.000180	0.301614
2.154242	-1.374061	0.275264	-0.000186	0.301429
1.519840	-1.289037	0.280269	-0.000068	0.301284
0.923175	-1.212824	0.285274	0.000043	0.301128
1.110473	-1.270567	0.290278	0.000008	0.301014
1.323390	-1.355783	0.295283	-0.000031	0.300790
1.304991	-1.364651	0.300288	-0.000028	0.300731
1.283801	-1.393835	0.305293	-0.000024	0.300571
1.689922	-1.496841	0.310298	-0.000099	0.300430
1.943365	-1.586697	0.315302	-0.000146	0.300219
2.089776	-1.658317	0.320307	-0.000173	0.300001
2.079928	-1.675696	0.325312	-0.000171	0.299909
2.139796	-1.753763	0.330317	-0.000182	0.299584
1.837088	-1.718093	0.335322	-0.000126	0.299490
1.825831	-1.756014	0.340326	-0.000124	0.299296
1.258408	-1.697901	0.345331	-0.000018	0.299078
1.062627	-1.686517	0.350336	0.000019	0.298961
1.485885	-1.826103	0.355341	-0.000060	0.298657
0.965204	-1.748635	0.360346	0.000037	0.298573
1.237787	-1.851991	0.365350	-0.000014	0.298312
1.796260	-1.991497	0.370355	-0.000118	0.298127
2.337695	-2.120467	0.375360	-0.000218	0.297978
2.480001	-2.211173	0.380365	-0.000244	0.297663
2.565532	-2.273031	0.385370	-0.000260	0.297437
2.281359	-2.257860	0.390374	-0.000207	0.297259
2.170634	-2.284551	0.395379	-0.000187	0.297031
1.806479	-2.268318	0.400384	-0.000119	0.296787
1.556601	-2.262995	0.405389	-0.000072	0.296591
1.103194	-2.214677	0.410394	0.000012	0.296425
0.796212	-2.221047	0.415398	0.000070	0.296121
0.056624	-2.115533	0.420403	0.000207	0.295979
0.192976	-2.170409	0.425408	0.000182	0.295831
0.589599	-2.291883	0.430413	0.000108	0.295589
0.777237	-2.360826	0.435418	0.000074	0.295418
0.858190	-2.415016	0.440422	0.000059	0.295224
0.795644	-2.471892	0.445427	0.000070	0.294889
0.043103	-2.364825	0.450432	0.000211	0.294743
-0.041994	-2.382276	0.455437	0.000227	0.294581
-0.285367	-2.394118	0.460442	0.000272	0.294305
-0.047770	-2.479395	0.465446	0.000228	0.294097
-0.443067	-2.444825	0.470451	0.000302	0.293914
-0.221080	-2.542566	0.475456	0.000260	0.293630
-0.285668	-2.575471	0.480461	0.000272	0.293410
-1.059891	-2.463947	0.485466	0.000417	0.293265
-1.009710	-2.521189	0.490470	0.000407	0.293027
-0.958045	-2.579855	0.495475	0.000398	0.292784
-1.417042	-2.526464	0.500480	0.000483	0.292635
-2.052217	-2.461949	0.505485	0.000602	0.292382
-2.139549	-2.484420	0.510490	0.000618	0.292192
-2.677824	-2.410165	0.515494	0.000718	0.292075
-2.722809	-2.458162	0.520499	0.000727	0.291796
-2.459341	-2.532344	0.525504	0.000678	0.291665
-3.224819	-2.439784	0.530509	0.000821	0.291433
-3.193026	-2.485123	0.535514	0.000815	0.291236
-3.580581	-2.437403	0.540518	0.000887	0.291123
-4.120799	-2.397502	0.545523	0.000988	0.290833
-3.988209	-2.431149	0.550528	0.000963	0.290785
-4.070073	-2.462527	0.555533	0.000978	0.290554
-3.995859	-2.505774	0.560538	0.000965	0.290405
-3.857254	-2.573762	0.565542	0.000939	0.290192
-3.828761	-2.628649	0.570547	0.000934	0.289943
-4.013972	-2.616651	0.575552	0.000968	0.289835
-4.158845	-2.651475	0.580557	0.000995	0.289529
-4.069017	-2.694326	0.585562	0.000979	0.289396
-4.800244	-2.589860	0.590566	0.001115	0.289253
-5.349999	-2.540444	0.595571	0.001217	0.289000
-5.591713	-2.511674	0.600576	0.001263	0.288923
-6.063464	-2.482451	0.605581	0.001350	0.288639
-6.117685	-2.481275	0.610586	0.001361	0.288595
-5.909241	-2.581288	0.615590	0.001322	0.288283
-6.314429	-2.518269	0.620595	0.001397	0.288229
-6.844556	-2.466553	0.625600	0.001496	0.288005
-6.707921	-2.508848	0.630605	0.001471	0.287917
-6.486464	-2.604747	0.635610	0.001430	0.287636
-6.884756	-2.550846	0.640614	0.001504	0.287543
-8.085963	-2.369091	0.645619	0.001728	0.287358
-6.881603	-2.615022	0.650624	0.001504	0.287222
-8.080161	-2.436124	0.655629	0.001727	0.287025
-7.767142	-2.516878	0.660634	0.001669	0.286904
-7.665603	-2.572938	0.665638	0.001650	0.286714
-7.834991	-2.570324	0.670643	0.001681	0.286571
-8.367382	-2.509933	0.675648	0.001781	0.286387
-8.146908	-2.575960	0.680653	0.001740	0.286255
-8.951604	-2.463129	0.685658	0.001890	0.286085
-8.092713	-2.645854	0.690662	0.001730	0.285951
-9.414742	-2.443264	0.695667	0.001976	0.285759
-9.473712	-2.440050	0.700672	0.001987	0.285720
-9.463149	-2.482601	0.705677	0.001985	0.285514
-9.535225	-2.477317	0.710682	0.001999	0.285474
-9.282716	-2.584986	0.715686	0.001952	0.285160
-9.566192	-2.536841	0.720691	0.002005	0.285143
-10.118734	-2.493959	0.725696	0.002108	0.284850
-11.016038	-2.327836	0.730701	0.002275	0.284865
-10.479196	-2.477179	0.735706	0.002175	0.284601
-11.151708	-2.364725	0.740710	0.002300	0.284551
-10.858832	-2.448196	0.745715	0.002246	0.284397
-10.902743	-2.469799	0.750720	0.002254	0.284246
-11.558635	-2.356349	0.755725	0.002376	0.284216
-11.622272	-2.406463	0.760730	0.002388	0.283901
-11.109353	-2.500413	0.765734	0.002293	0.283897
-11.529197	-2.473310	0.770739	0.002371	0.283645
-11.893889	-2.415808	0.775744	0.002439	0.283600
-11.799890	-2.466107	0.780749	0.002422	0.283430
-12.447346	-2.378820	0.785754	0.002542	0.283274
-12.627977	-2.343269	0.790758	0.002576	0.283287
-13.434977	-2.251403	0.795763	0.002726	0.283007
-12.608735	-2.404549	0.800768	0.002573	0.282991
-12.107346	-2.533216	0.805773	0.002479	0.282799
-12.849123	-2.430935	0.810778	0.002617	0.282632
-12.771885	-2.454985	0.815782	0.002603	0.282580
-12.994682	-2.466075	0.820787	0.002645	0.282315
-12.865563	-2.488647	0.825792	0.002621	0.282319
-13.586969	-2.411061	0.830797	0.002755	0.282044
-14.063933	-2.329404	0.835802	0.002844	0.282018
-13.608145	-2.431250	0.840806	0.002759	0.281920
-14.352977	-2.335580	0.845811	0.002898	0.281715
-13.801445	-2.435856	0.850816	0.002796	0.281715
-13.787422	-2.493855	0.855821	0.002793	0.281429
-14.721139	-2.332341	0.860826	0.002967	0.281386
-14.637598	-2.366249	0.865830	0.002951	0.281289
-14.199056	-2.491984	0.870835	0.002870	0.281052
-14.016015	-2.523717	0.875840	0.002836	0.281060
-14.620586	-2.475464	0.880845	0.002949	0.280742
-14.644054	-2.471202	0.885850	0.002953	0.280741
-14.629484	-2.498483	0.890854	0.002950	0.280614
-15.326913	-2.392711	0.895859	0.003080	0.280505
-14.929625	-2.475711	0.900864	0.003006	0.280449
-15.246853	-2.470470	0.905869	0.003066	0.280177
-15.563716	-2.412255	0.910874	0.003125	0.280180
-16.246372	-2.329819	0.915878	0.003252	0.279964
-16.647065	-2.272876	0.920883	0.003326	0.279881
-16.212360	-2.352128	0.925888	0.003246	0.279880
-16.392105	-2.386271	0.930893	0.003279	0.279534
-16.509338	-2.363143	0.935898	0.003301	0.279542
-16.239114	-2.434462	0.940902	0.003251	0.279427
-17.163191	-2.298853	0.945907	0.003423	0.279259
-16.951232	-2.336677	0.950912	0.003384	0.279262
-16.986211	-2.378340	0.955917	0.003390	0.279012
-16.974116	-2.400085	0.960922	0.003388	0.278911
-16.953694	-2.415126	0.965926	0.003384	0.278851
-17.118531	-2.434393	0.970931	0.003415	0.278595
-17.336233	-2.391329	0.975936	0.003456	0.278613
-17.966985	-2.317790	0.980941	0.003573	0.278398
-17.894465	-2.354175	0.985946	0.003560	0.278277
-17.291930	-2.466265	0.990950	0.003448	0.278264
-18.075669	-2.375680	0.995955	0.003594	0.277993
-17.706252	-2.443125	1.000960	0.003525	0.277991
-17.874552	-2.446175	1.005965	0.003557	0.277815
-18.222731	-2.413399	1.010970	0.003622	0.277656
-18.595119	-2.342505	1.015974	0.003691	0.277672
-18.989731	-2.333274	1.020979	0.003764	0.277345
-18.727272	-2.379188	1.025984	0.003716	0.277354
-18.758986	-2.395746	1.030989	0.003722	0.277237
-18.727965	-2.444926	1.035994	0.003716	0.277009
-18.645347	-2.458307	1.040998	0.003701	0.277018
-19.327779	-2.382108	1.046003	0.003828	0.276767
-19.403596	-2.374789	1.051008	0.003842	0.276732
-19.151466	-2.439434	1.056013	0.003795	0.276634
-19.687674	-2.386904	1.061018	0.003895	0.276398
-19.533945	-2.413957	1.066022	0.003867	0.276402
-20.477144	-2.280952	1.071027	0.004042	0.276200
-20.002170	-2.386997	1.076032	0.003954	0.276096
-20.167412	-2.358239	1.081037	0.003985	0.276089
-21.206930	-2.223254	1.086042	0.004178	0.275805
-20.827284	-2.292006	1.091046	0.004108	0.275806
-21.151241	-2.235320	1.096051	0.004168	0.275794
-21.019387	-2.305917	1.101056	0.004144	0.275549
-21.087919	-2.295259	1.106061	0.004157	0.275539
-21.132082	-2.302878	1.111066	0.004165	0.275456
-21.146265	-2.348815	1.116070	0.004168	0.275200
-21.286524	-2.324391	1.121075	0.004194	0.275194
-21.456215	-2.324841	1.126080	0.004226	0.275029
-21.840160	-2.283142	1.131085	0.004297	0.274880
-21.178929	-2.407802	1.136090	0.004174	0.274857
-21.240408	-2.449628	1.141094	0.004186	0.274577
-21.368251	-2.435870	1.146099	0.004210	0.274526
-21.623131	-2.410652	1.151104	0.004257	0.274415
-21.798295	-2.411843	1.156109	0.004290	0.274240
-21.495232	-2.468114	1.161114	0.004234	0.274233
-21.882977	-2.459470	1.166118	0.004306	0.273906
-22.606305	-2.329018	1.171123	0.004441	0.273900
-22.098347	-2.446184	1.176128	0.004346	0.273768
-22.546905	-2.396474	1.181133	0.004430	0.273599
-22.392472	-2.426458	1.186138	0.004401	0.273589
-22.276872	-2.503114	1.191142	0.004380	0.273294
-22.858822	-2.400015	1.196147	0.004488	0.273279
-22.592139	-2.477933	1.201152	0.004439	0.273122
-23.049876	-2.421617	1.206157	0.004524	0.272979
-22.864304	-2.457933	1.211162	0.004489	0.272965
-23.083131	-2.476757	1.216166	0.004530	0.272653
-23.424571	-2.415703	1.221171	0.004594	0.272647
-23.548327	-2.424617	1.226176	0.004617	0.272480
-24.315692	-2.305894	1.231181	0.004760	0.272369
-24.516687	-2.271632	1.236186	0.004797	0.272356
-24.243177	-2.370524	1.241190	0.004747	0.272094
-24.437188	-2.348089	1.246195	0.004783	0.272026
-24.331910	-2.377939	1.251200	0.004763	0.271968
-24.537062	-2.385716	1.256205	0.004802	0.271728
-24.773991	-2.341379	1.261210	0.004846	0.271734
-24.914501	-2.348240	1.266214	0.004872	0.271560
-25.367053	-2.297049	1.271219	0.004956	0.271394
-25.072492	-2.347298	1.276224	0.004902	0.271411
-25.439744	-2.323852	1.281229	0.004970	0.271180
-25.927916	-2.249034	1.286234	0.005061	0.271105
-25.618922	-2.302771	1.291238	0.005004	0.271117
-25.488534	-2.390220	1.296243	0.004979	0.270776
-25.357246	-2.414899	1.301248	0.004955	0.270771
-26.199866	-2.277323	1.306253	0.005112	0.270687
-26.364159	-2.276393	1.311258	0.005143	0.270532
-26.217607	-2.300128	1.316262	0.005115	0.270547
-27.084083	-2.180709	1.321267	0.005277	0.270342
-26.915190	-2.238067	1.326272	0.005246	0.270199
-26.720031	-2.273921	1.331277	0.005209	0.270197
-27.174879	-2.230957	1.336282	0.005294	0.269983
-27.568902	-2.176591	1.341286	0.005367	0.269890
-26.567780	-2.365178	1.346291	0.005181	0.269854
-26.797640	-2.373820	1.351296	0.005224	0.269583
-27.345733	-2.282711	1.356301	0.005326	0.269536
-26.839512	-2.388491	1.361306	0.005232	0.269462
-27.039794	-2.391278	1.366310	0.005270	0.269251
-28.019416	-2.211534	1.371315	0.005452	0.269259
-27.382419	-2.365877	1.376320	0.005333	0.269052
-28.156481	-2.246212	1.381325	0.005478	0.268937
-27.760572	-2.322789	1.386330	0.005404	0.268912
-28.409463	-2.252365	1.391334	0.005525	0.268656
-28.217715	-2.297689	1.396339	0.005489	0.268599
-28.137909	-2.321819	1.401344	0.005475	0.268546
-28.619457	-2.283465	1.406349	0.005564	0.268280
-28.430735	-2.317734	1.411354	0.005529	0.268280
-28.591950	-2.312878	1.416358	0.005559	0.268148
-29.217908	-2.226455	1.421363	0.005676	0.267999
-28.760080	-2.310108	1.426368	0.005591	0.267997
-28.965647	-2.320774	1.431373	0.005629	0.267736
-29.270825	-2.281442	1.436378	0.005686	0.267648
-29.124879	-2.313604	1.441382	0.005659	0.267617
-29.685230	-2.260707	1.446387	0.005763	0.267352
-30.028953	-2.194794	1.451392	0.005827	0.267370
-29.991334	-2.220300	1.456397	0.005821	0.267268
-29.934782	-2.277327	1.461402	0.005810	0.267014
-29.730981	-2.310072	1.466406	0.005772	0.267037
-30.892176	-2.124812	1.471411	0.005989	0.266896
-30.827020	-2.160485	1.476416	0.005976	0.266766
-30.814988	-2.160448	1.481421	0.005974	0.266778
-31.489375	-2.064338	1.486426	0.006100	0.266633
-31.282236	-2.139657	1.491430	0.006061	0.266428
-30.939637	-2.204214	1.496435	0.005998	0.266416
-31.301389	-2.159332	1.501440	0.006065	0.266301
-31.490971	-2.159879	1.506445	0.006101	0.266110
-31.087928	-2.235124	1.511450	0.006026	0.266099
-31.012117	-2.283446	1.516454	0.006012	0.265911
-31.698658	-2.182335	1.521459	0.006140	0.265781
-31.635094	-2.191619	1.526464	0.006128	0.265793
-31.232789	-2.308540	1.531469	0.006053	0.265554
-31.639839	-2.241121	1.536474	0.006129	0.265517
-31.006444	-2.380769	1.541478	0.006011	0.265384
-31.437610	-2.342914	1.546483	0.006092	0.265162
-31.204509	-2.384565	1.551488	0.006048	0.265165
-31.757849	-2.339851	1.556493	0.006151	0.264859
-32.666794	-2.173068	1.561498	0.006321	0.264867
-32.138146	-2.286635	1.566502	0.006222	0.264771
-32.971038	-2.176059	1.571507	0.006377	0.264547
-33.148458	-2.142716	1.576512	0.006410	0.264552
-32.814718	-2.230262	1.581517	0.006348	0.264405
-32.917645	-2.239551	1.586522	0.006368	0.264251
-32.388957	-2.336590	1.591526	0.006269	0.264245
-33.073631	-2.270757	1.596531	0.006397	0.263923
-32.638264	-2.353803	1.601536	0.006316	0.263901
-32.434194	-2.420582	1.606541	0.006278	0.263738
-33.157859	-2.317182	1.611546	0.006413	0.263582
-33.015797	-2.343666	1.616550	0.006387	0.263578
-34.269138	-2.167774	1.621555	0.006620	0.263292
-34.053240	-2.208083	1.626560	0.006580	0.263285
-34.144655	-2.203641	1.631565	0.006597	0.263218
-33.993931	-2.272393	1.636570	0.006569	0.262990
-34.244321	-2.223821	1.641574	0.006616	0.263006
-34.557460	-2.209745	1.646579	0.006674	0.262769
-34.451498	-2.247767	1.651584	0.006654	0.262666
-34.562640	-2.228252	1.656589	0.006675	0.262661
-34.894580	-2.226286	1.661594	0.006737	0.262338
-34.531111	-2.291584	1.666598	0.006670	0.262343
-34.792035	-2.268607	1.671603	0.006718	0.262207
-34.973765	-2.270714	1.676608	0.006752	0.262012
-34.995370	-2.265696	1.681613	0.006756	0.262018
-35.451205	-2.225095	1.686618	0.006841	0.261783
-35.699564	-2.186072	1.691622	0.006888	0.261749
-35.556225	-2.223896	1.696627	0.006861	0.261683
-36.024924	-2.186937	1.701632	0.006948	0.261415
-36.288404	-2.139004	1.706637	0.006997	0.261415
-36.557826	-2.105824	1.711642	0.007048	0.261326
-36.218500	-2.206325	1.716646	0.006985	0.261111
-36.637162	-2.129799	1.721651	0.007063	0.261113
-36.636281	-2.160477	1.726656	0.007063	0.260943
-36.817652	-2.154829	1.731661	0.007096	0.260790
-36.734828	-2.169129	1.736666	0.007081	0.260794
-37.173452	-2.120756	1.741670	0.007163	0.260619
-37.554436	-2.064063	1.746675	0.007234	0.260549
-37.162937	-2.132549	1.751680	0.007161	0.260563
-37.119119	-2.198351	1.756685	0.007153	0.260241
-37.627296	-2.111934	1.761690	0.007248	0.260207
-37.474520	-2.149345	1.766694	0.007219	0.260153
-37.691982	-2.157919	1.771699	0.007260	0.259885
-37.422604	-2.208166	1.776704	0.007210	0.259877
-37.827686	-2.162157	1.781709	0.007285	0.259722
-38.043130	-2.152324	1.786714	0.007326	0.259558
-38.042438	-2.151496	1.791718	0.007326	0.259563
-38.257347	-2.157780	1.796723	0.007366	0.259309
-38.359830	-2.144209	1.801728	0.007385	0.259280
-38.840853	-2.059209	1.806733	0.007474	0.259266
-39.322676	-2.028345	1.811738	0.007564	0.258948
-38.439341	-2.190835	1.816742	0.007400	0.258937
-38.665554	-2.169078	1.821747	0.007442	0.258828
-38.856225	-2.173053	1.826752	0.007478	0.258612
-38.786918	-2.185820	1.831757	0.007465	0.258610
-39.142830	-2.161001	1.836762	0.007531	0.258386
-39.396926	-2.127796	1.841766	0.007579	0.258312
-39.285206	-2.155012	1.846771	0.007558	0.258273
-39.023016	-2.253236	1.851776	0.007509	0.257989
-38.911761	-2.272852	1.856781	0.007489	0.257992
-39.432207	-2.215746	1.861786	0.007586	0.257781
-39.304887	-2.259510	1.866790	0.007562	0.257665
-39.257381	-2.282305	1.871795	0.007553	0.257585
-40.010737	-2.185822	1.876800	0.007694	0.257356
-40.163586	-2.157425	1.881805	0.007722	0.257359
-39.903512	-2.246159	1.886810	0.007674	0.257125
-40.580922	-2.137614	1.891814	0.007800	0.257042
-40.864519	-2.088674	1.896819	0.007853	0.257026
-40.815501	-2.145154	1.901824	0.007844	0.256758
-40.462487	-2.211639	1.906829	0.007778	0.256744
-40.845959	-2.172172	1.911834	0.007850	0.256573
-41.125244	-2.148444	1.916838	0.007902	0.256419
-41.048239	-2.161857	1.921843	0.007887	0.256422
-41.822963	-2.064665	1.926848	0.008032	0.256175
-41.771696	-2.084010	1.931853	0.008022	0.256117
-41.178224	-2.205872	1.936858	0.007912	0.256038
-41.348240	-2.218475	1.941862	0.007944	0.255791
-41.607459	-2.173708	1.946867	0.007992	0.255777
-41.310570	-2.258436	1.951872	0.007937	0.255603
-41.574385	-2.223455	1.956877	0.007986	0.255529
-41.396125	-2.277817	1.961882	0.007953	0.255404
-42.043922	-2.195907	1.966886	0.008074	0.255199
-41.914423	-2.220434	1.971891	0.008050	0.255193
-42.334960	-2.191714	1.976896	0.008128	0.254922
-42.435153	-2.181197	1.981901	0.008147	0.254877
-42.158068	-2.255636	1.986906	0.008095	0.254740
-42.762975	-2.174756	1.991910	0.008208	0.254574
-42.999082	-2.134976	1.996915	0.008252	0.254555
-42.296090	-2.315061	2.001920	0.008121	0.254258

-42.599164	-2.307042	2.011917	0.008178	0.253988
-42.622351	-2.341868	2.021914	0.008182	0.253764
-43.606253	-2.189551	2.031910	0.008366	0.253611
-43.256804	-2.298895	2.041907	0.008301	0.253348
-43.885804	-2.192908	2.051904	0.008418	0.253299
-43.984407	-2.218720	2.061901	0.008437	0.253048
-43.803637	-2.260190	2.071898	0.008403	0.252998
-44.263385	-2.196556	2.081894	0.008489	0.252882
-44.017423	-2.282881	2.091891	0.008443	0.252643
-43.794377	-2.323583	2.101888	0.008402	0.252641
-43.798546	-2.328350	2.111885	0.008403	0.252608
-44.068107	-2.328147	2.121882	0.008453	0.252327
-43.937162	-2.353608	2.131878	0.008429	0.252317
-44.077981	-2.326184	2.141875	0.008456	0.252326
-44.317867	-2.281003	2.151872	0.008500	0.252334
-44.330236	-2.279510	2.161869	0.008503	0.252329
-43.843853	-2.371347	2.171866	0.008413	0.252309
-44.055106	-2.332066	2.181862	0.008452	0.252312
-43.599089	-2.415557	2.191859	0.008367	0.252308
-43.827680	-2.373074	2.201856	0.008410	0.252313
-43.904028	-2.358731	2.211853	0.008424	0.252314
-43.790538	-2.379149	2.221850	0.008404	0.252314
-44.111401	-2.319332	2.231846	0.008463	0.252322
-43.797980	-2.376628	2.241843	0.008405	0.252319
-43.819294	-2.373283	2.251840	0.008409	0.252315
-43.816294	-2.372674	2.261837	0.008409	0.252321
-43.444708	-2.413996	2.271834	0.008340	0.252471
-43.408211	-2.394577	2.281830	0.008333	0.252619
-43.275422	-2.418444	2.291827	0.008309	0.252620
-43.645596	-2.348611	2.301824	0.008378	0.252633
-43.587034	-2.324557	2.311821	0.008367	0.252831
-43.474284	-2.319320	2.321818	0.008346	0.252978
-43.278192	-2.355851	2.331814	0.008310	0.252972
-43.143066	-2.339233	2.341811	0.008285	0.253207
-43.335689	-2.292339	2.351808	0.008321	0.253273
-43.286854	-2.277089	2.361805	0.008312	0.253410
-43.142561	-2.271375	2.371802	0.008285	0.253592
-43.432045	-2.196417	2.381798	0.008339	0.253718
-42.738308	-2.289461	2.391795	0.008211	0.253907
-42.930740	-2.225774	2.401792	0.008246	0.254069
-42.413533	-2.289768	2.411789	0.008150	0.254240
-42.303285	-2.281462	2.421786	0.008130	0.254400
-41.979917	-2.319797	2.431782	0.008070	0.254516
-42.313978	-2.214031	2.441779	0.008132	0.254771
-42.178501	-2.219112	2.451776	0.008107	0.254881
-41.484904	-2.294597	2.461773	0.007978	0.255168
-41.965788	-2.182133	2.471770	0.008068	0.255309
-41.085967	-2.307556	2.481766	0.007904	0.255505
-41.393344	-2.218400	2.491763	0.007962	0.255692
-41.251625	-2.221278	2.501760	0.007936	0.255821
-40.765550	-2.262603	2.511757	0.007845	0.256086
-40.968131	-2.190250	2.521754	0.007883	0.256286
-40.468534	-2.257660	2.531750	0.007790	0.256418
-40.239310	-2.246017	2.541747	0.007748	0.256718
-40.186241	-2.224469	2.551744	0.007738	0.256893
-39.773796	-2.274140	2.561741	0.007661	0.257035
-40.084958	-2.162362	2.571738	0.007720	0.257345
-39.641375	-2.200860	2.581734	0.007637	0.257581
-39.733136	-2.146279	2.591731	0.007654	0.257793
-38.931431	-2.255494	2.601728	0.007505	0.257998
-38.567038	-2.276374	2.611725	0.007438	0.258252
-38.736710	-2.215741	2.621722	0.007469	0.258418
-38.001204	-2.318494	2.631718	0.007333	0.258591
-38.067715	-2.251506	2.641715	0.007345	0.258897
-37.669721	-2.292601	2.651712	0.007271	0.259071
-37.280954	-2.330594	2.661709	0.007199	0.259253
-37.834187	-2.177699	2.671706	0.007302	0.259544
-37.420840	-2.210369	2.681702	0.007225	0.259780
-37.365231	-2.179322	2.691699	0.007215	0.260009
-36.954927	-2.215949	2.701696	0.007139	0.260219
-36.761441	-2.193768	2.711693	0.007103	0.260538
-36.736305	-2.166100	2.721690	0.007099	0.260716
-36.504352	-2.168678	2.731686	0.007056	0.260935
-36.418244	-2.141629	2.741683	0.007040	0.261171
-35.633326	-2.244374	2.751680	0.006894	0.261392
-35.791007	-2.159378	2.761677	0.006923	0.261703
-35.828891	-2.110717	2.771674	0.006931	0.261933
-35.288324	-2.166403	2.781670	0.006830	0.262168
-34.940115	-2.187765	2.791667	0.006765	0.262398
-34.189995	-2.278027	2.801664	0.006626	0.262652
-34.313803	-2.206342	2.811661	0.006649	0.262922
-33.910193	-2.244454	2.821658	0.006574	0.263116
-33.939584	-2.197557	2.831654	0.006580	0.263343
-33.968086	-2.142553	2.841651	0.006585	0.263616
-33.532908	-2.168507	2.851648	0.006504	0.263907
-32.832270	-2.254498	2.861645	0.006374	0.264134
-32.632376	-2.255342	2.871642	0.006337	0.264328
-32.470244	-2.249034	2.881638	0.006307	0.264523
-32.741571	-2.136805	2.891635	0.006358	0.264866
-32.007572	-2.228664	2.901632	0.006221	0.265092
-31.554619	-2.270477	2.911629	0.006137	0.265313
-31.226760	-2.292675	2.921626	0.006076	0.265516
-31.349725	-2.221977	2.931622	0.006099	0.265779
-31.120307	-2.220755	2.941619	0.006057	0.266012
-30.420049	-2.314381	2.951616	0.005927	0.266195
-30.725119	-2.216607	2.961613	0.005984	0.266424
-30.342115	-2.227114	2.971610	0.005912	0.266744
-30.079003	-2.235062	2.981606	0.005864	0.266960
-29.817252	-2.245733	2.991603	0.005815	0.267159
-29.430082	-2.273383	3.001600	0.005743	0.267390
-29.309569	-2.244185	3.011597	0.005721	0.267666
-29.323495	-2.188508	3.021594	0.005724	0.267952
-29.116448	-2.184781	3.031590	0.005685	0.268175
-28.378496	-2.282642	3.041587	0.005548	0.268370
-27.759818	-2.353254	3.051584	0.005433	0.268595
-28.049411	-2.248061	3.061581	0.005487	0.268877
-27.685334	-2.272398	3.071578	0.005420	0.269102
-27.753171	-2.218111	3.081574	0.005432	0.269326
-27.690435	-2.185631	3.091571	0.005421	0.269561
-27.289729	-2.197695	3.101568	0.005346	0.269887
-27.291350	-2.151035	3.111565	0.005347	0.270135
-26.941960	-2.162981	3.121562	0.005282	0.270410
-27.079688	-2.092042	3.131558	0.005308	0.270655
-26.599150	-2.137548	3.141555	0.005218	0.270878
-26.280537	-2.148327	3.151552	0.005159	0.271129
-26.273974	-2.090310	3.161549	0.005158	0.271444
-26.043302	-2.079371	3.171546	0.005115	0.271725
-25.499415	-2.134736	3.181542	0.005014	0.271956
-24.809643	-2.220746	3.191539	0.004886	0.272165
-24.616916	-2.210582	3.201536	0.004850	0.272405
-23.966621	-2.277638	3.211533	0.004730	0.272676
-23.852428	-2.250580	3.221530	0.004709	0.272929
-23.898096	-2.203922	3.231526	0.004717	0.273131
-23.645164	-2.207349	3.241523	0.004670	0.273356
-23.292572	-2.219920	3.251520	0.004605	0.273628
-23.051389	-2.214118	3.261517	0.004560	0.273890
-22.667563	-2.241153	3.271514	0.004489	0.274115
-22.575560	-2.217673	3.281510	0.004472	0.274326
-22.148888	-2.251096	3.291507	0.004393	0.274558
-21.761760	-2.268891	3.301504	0.004321	0.274835
-22.059529	-2.171601	3.311501	0.004376	0.275061
-21.537165	-2.220379	3.321498	0.004279	0.275303
-21.492770	-2.180860	3.331494	0.004271	0.275552
-20.977260	-2.229498	3.341491	0.004175	0.275788
-20.795825	-2.221178	3.351488	0.004142	0.276004
-20.199602	-2.293708	3.361485	0.004031	0.276192
-20.161069	-2.259956	3.371482	0.004024	0.276404
-20.404926	-2.150251	3.381478	0.004069	0.276745
-19.582667	-2.261618	3.391475	0.003916	0.276944
-19.465001	-2.244217	3.401472	0.003895	0.277146
-19.270433	-2.235078	3.411469	0.003859	0.277377
-19.093694	-2.210833	3.421466	0.003826	0.277671
-18.957206	-2.183194	3.431462	0.003801	0.277943
-18.504587	-2.224360	3.441459	0.003717	0.278156
-18.257939	-2.231264	3.451456	0.003671	0.278353
-18.069306	-2.213961	3.461453	0.003636	0.278620
-17.869909	-2.198119	3.471450	0.003599	0.278890
-17.649052	-2.194314	3.481446	0.003558	0.279117
-17.465421	-2.179278	3.491443	0.003524	0.279367
-17.425260	-2.142080	3.501440	0.003517	0.279597
-16.612673	-2.235228	3.511437	0.003366	0.279879
-16.580643	-2.192803	3.521434	0.003360	0.280127
-16.475529	-2.165103	3.531430	0.003340	0.280368
-16.288567	-2.154434	3.541427	0.003306	0.280598
-15.658180	-2.235331	3.551424	0.003189	0.280771
-15.333703	-2.237206	3.561421	0.003128	0.281064
-15.464408	-2.171656	3.571418	0.003153	0.281278
-15.156387	-2.184376	3.581414	0.003096	0.281500
-14.662801	-2.228973	3.591411	0.003004	0.281731
-14.321010	-2.235134	3.601408	0.002940	0.282018
-13.964760	-2.258328	3.611405	0.002874	0.282231
-14.020204	-2.208314	3.621402	0.002885	0.282434
-13.940942	-2.175865	3.631398	0.002870	0.282674
-13.450747	-2.200641	3.641395	0.002779	0.283002
-13.062496	-2.232871	3.651392	0.002707	0.283197
-13.187481	-2.164239	3.661389	0.002730	0.283431
-13.176306	-2.117001	3.671386	0.002728	0.283682
-12.595812	-2.171337	3.681382	0.002621	0.283942
-12.319264	-2.165050	3.691379	0.002569	0.284229
-12.286274	-2.128090	3.701376	0.002563	0.284447
-12.403435	-2.056347	3.711373	0.002585	0.284703
-12.029566	-2.074429	3.721370	0.002516	0.284955
-11.623568	-2.095978	3.731366	0.002440	0.285220
-11.474051	-2.056561	3.741363	0.002413	0.285557
-10.965762	-2.110518	3.751360	0.002318	0.285751
-10.755698	-2.104408	3.761357	0.002279	0.285974
-10.335990	-2.138954	3.771354	0.002201	0.286185
-9.630180	-2.220639	3.781350	0.002070	0.286419
-9.444229	-2.200307	3.791347	0.002036	0.286692
-8.998260	-2.248056	3.801344	0.001953	0.286859
-9.043491	-2.200436	3.811341	0.001961	0.287057
-8.899135	-2.162104	3.821338	0.001935	0.287382
-8.619433	-2.169726	3.831334	0.001883	0.287598
-8.627106	-2.124117	3.841331	0.001884	0.287820
-8.162749	-2.162255	3.851328	0.001798	0.288052
-7.964949	-2.145371	3.861325	0.001761	0.288316
-7.626027	-2.159079	3.871322	0.001699	0.288556
-7.545442	-2.128801	3.881318	0.001684	0.288780
-7.071956	-2.175457	3.891315	0.001596	0.288977
-7.020353	-2.121141	3.901312	0.001586	0.289295
-6.749222	-2.124913	3.911309	0.001536	0.289522
-5.936036	-2.236160	3.921306	0.001385	0.289703
-6.073771	-2.167877	3.931302	0.001411	0.289919
-5.923579	-2.134071	3.941299	0.001383	0.290223
-5.627783	-2.138062	3.951296	0.001328	0.290470
-5.349537	-2.151892	3.961293	0.001276	0.290652
-5.425912	-2.098058	3.971290	0.001291	0.290850
-5.028525	-2.115503	3.981286	0.001217	0.291122
-4.874742	-2.093023	3.991283	0.001188	0.291371
-4.354661	-2.143588	4.001280	0.001092	0.291589
-4.370638	-2.093785	4.011277	0.001095	0.291821
-4.283553	-2.062896	4.021274	0.001079	0.292051
-4.313271	-1.994120	4.031270	0.001084	0.292364
-4.264231	-1.949441	4.041267	0.001075	0.292629
-3.743384	-1.991076	4.051264	0.000979	0.292890
-3.640721	-1.957398	4.061261	0.000960	0.293148
-3.872079	-1.859536	4.071258	0.001003	0.293422
-3.586599	-1.854119	4.081254	0.000950	0.293704
-3.396790	-1.830622	4.091251	0.000915	0.293989
-2.989077	-1.844411	4.101248	0.000839	0.294285
-2.548178	-1.869380	4.111245	0.000757	0.294555
-2.462810	-1.827694	4.121242	0.000741	0.294835
-2.010136	-1.856480	4.131238	0.000657	0.295097
-2.426762	-1.716869	4.141235	0.000735	0.295409
-2.326377	-1.677830	4.151232	0.000716	0.295688
-2.692837	-1.546872	4.161229	0.000785	0.296002
-2.434779	-1.527275	4.171226	0.000737	0.296326
-1.697573	-1.598431	4.181222	0.000600	0.296632
-1.692237	-1.536615	4.191219	0.000599	0.296938
-1.856189	-1.439821	4.201216	0.000629	0.297263
-1.381101	-1.458820	4.211213	0.000541	0.297590
-1.204990	-1.419159	4.221210	0.000509	0.297937
-1.308510	-1.332624	4.231206	0.000528	0.298265
-1.386387	-1.243873	4.241203	0.000543	0.298626
-1.130528	-1.211431	4.251200	0.000495	0.299008
-0.802098	-1.198015	4.261197	0.000434	0.299360
-0.835939	-1.121049	4.271194	0.000441	0.299702
-1.255268	-0.962484	4.281190	0.000519	0.300098
-0.765800	-0.971704	4.291187	0.000428	0.300482
-0.691901	-0.910508	4.301184	0.000414	0.300840
-0.318210	-0.900258	4.311181	0.000345	0.301215
-0.408014	-0.802781	4.321178	0.000362	0.301604
-0.374581	-0.730095	4.331174	0.000355	0.301980
-0.391712	-0.630013	4.341171	0.000359	0.302444
-0.240589	-0.570852	4.351168	0.000331	0.302857
-0.298643	-0.471391	4.361165	0.000342	0.303281
-0.256569	-0.381212	4.371162	0.000334	0.303746
0.392949	-0.416486	4.381158	0.000213	0.304140
0.026271	-0.249615	4.391155	0.000282	0.304615
0.155903	-0.180103	4.401152	0.000258	0.305056
0.142764	-0.072718	4.411149	0.000260	0.305553
0.000000	0.040538	4.421146	0.000287	0.305965

-0.204511	0.349445	4.426150	0.000325	0.307248
0.255452	0.813955	4.431155	0.000239	0.309818
0.471488	1.613752	4.436160	0.000198	0.313711
0.402936	2.747198	4.441165	0.000210	0.318840
1.166978	4.006341	4.446170	0.000067	0.325121
1.819363	5.595057	4.451174	-0.000055	0.332632
2.106040	7.542819	4.456179	-0.000110	0.341220
2.362985	9.809546	4.461184	-0.000159	0.350892
3.284457	12.254045	4.466189	-0.000332	0.361500
3.696492	15.120900	4.471194	-0.000410	0.373088
3.990752	18.337604	4.476198	-0.000467	0.385560
4.756320	21.793845	4.481203	-0.000612	0.398822
5.469111	25.609682	4.486208	-0.000747	0.412885
6.230215	29.763219	4.491213	-0.000891	0.427657
7.382795	34.187600	4.496218	-0.001109	0.443053
8.404707	39.002478	4.501222	-0.001302	0.459088
9.732094	44.112423	4.506227	-0.001553	0.475647
9.949369	49.783037	4.511232	-0.001597	0.492707
11.499837	55.547086	4.516237	-0.001889	0.510142
12.453008	61.766401	4.521242	-0.002070	0.527954
13.759433	68.247053	4.526246	-0.002318	0.546044
14.868655	75.078133	4.531251	-0.002529	0.564361
15.690218	82.285503	4.536256	-0.002686	0.582907
16.843460	89.709903	4.541261	-0.002906	0.601545
17.806872	97.440061	4.546266	-0.003090	0.620256
19.408847	105.325782	4.551270	-0.003394	0.639029
20.845855	113.478383	4.556275	-0.003666	0.657787
21.851427	121.938252	4.561280	-0.003859	0.676515
23.373111	130.490436	4.566285	-0.004148	0.695122
24.820424	139.242846	4.571290	-0.004423	0.713621
26.587293	148.110666	4.576294	-0.004758	0.731992
32.589581	156.411503	4.581299	-0.005881	0.750270
35.189293	165.480367	4.586304	-0.006370	0.768416
37.064418	174.814829	4.591309	-0.006726	0.786393
38.033620	184.380559	4.596314	-0.006912	0.804094
39.920291	193.859544	4.601318	-0.007270	0.821546
42.611970	203.256351	4.606323	-0.007777	0.838737
46.588989	212.472344	4.611328	-0.008523	0.855658
49.760284	221.918809	4.616333	-0.009120	0.872394
51.183357	231.687440	4.621338	-0.009391	0.888836
53.046515	241.390800	4.626342	-0.009744	0.904998
54.841965	251.082510	4.631347	-0.010085	0.920837
57.398911	260.625789	4.636352	-0.010567	0.936385
64.187161	269.460160	4.641357	-0.011837	0.951724
74.598068	277.739724	4.646362	-0.013780	0.966931
88.209036	285.659781	4.651366	-0.016320	0.982187
96.750480	294.594877	4.656371	-0.017916	0.997392
100.667512	304.293662	4.661376	-0.018652	1.012303
102.194745	314.361063	4.666381	-0.018942	1.026930
103.484407	324.341789	4.671386	-0.019189	1.041174
105.493021	334.098619	4.676390	-0.019569	1.055088
107.360071	343.807271	4.681395	-0.019923	1.068722
111.864255	352.975779	4.686400	-0.020768	1.082070
113.677785	362.576884	4.691405	-0.021112	1.095211
115.811601	372.011756	4.696410	-0.021515	1.108050
117.933887	381.381881	4.701414	-0.021916	1.120655
118.776315	390.908582	4.706419	-0.022079	1.133038
121.273986	400.049918	4.711424	-0.022550	1.145159
122.836685	409.306924	4.716429	-0.022847	1.157096
123.960969	418.541247	4.721434	-0.023062	1.168789
126.007871	427.549757	4.726438	-0.023449	1.180283
127.211562	436.651322	4.731443	-0.023679	1.191603
129.479963	445.482519	4.736448	-0.024107	1.202710
131.425417	454.366289	4.741453	-0.024475	1.213710
131.819694	463.466732	4.746458	-0.024554	1.224556
132.788461	472.395243	4.751462	-0.024740	1.235219
134.221630	481.148745	4.756467	-0.025013	1.245679
135.534308	489.925934	4.761472	-0.025263	1.256055
136.245080	498.755535	4.766477	-0.025401	1.266289
137.289473	507.469306	4.771482	-0.025601	1.276373
138.883906	516.050514	4.776486	-0.025903	1.286334
139.424987	524.810172	4.781491	-0.026010	1.296218
140.217371	533.473814	4.786496	-0.026163	1.305967
141.263370	542.136972	4.791501	-0.026363	1.315690
142.067166	550.687352	4.796506	-0.026518	1.325175
143.684397	559.102510	4.801510	-0.026825	1.334593
144.859901	567.576262	4.806515	-0.027049	1.343927
145.634315	576.127024	4.811520	-0.027199	1.353208
147.366159	584.449803	4.816525	-0.027527	1.362352
148.523854	592.903310	4.821530	-0.027748	1.371472
149.261636	601.433519	4.826534	-0.027891	1.380538
150.223336	609.877437	4.831539	-0.028075	1.389494
151.296864	618.279930	4.836544	-0.028280	1.398368
152.080787	626.718824	4.841549	-0.028432	1.407174
152.665915	635.169201	4.846554	-0.028546	1.415903
153.622680	643.530030	4.851558	-0.028730	1.424550
154.506760	651.897259	4.856563	-0.028900	1.433138
155.251426	660.287066	4.861568	-0.029044	1.441675
156.032568	668.652160	4.866573	-0.029194	1.450142
156.523283	677.048661	4.871578	-0.029291	1.458544
157.572066	685.335189	4.876582	-0.029492	1.466880
158.384730	693.676404	4.881587	-0.029648	1.475183
158.560340	702.104140	4.886592	-0.029687	1.483423
159.436977	710.378712	4.891597	-0.029855	1.491579
160.348534	718.616457	4.896602	-0.030030	1.499661
161.321213	726.876522	4.901606	-0.030216	1.507731
161.433302	735.286404	4.906611	-0.030243	1.515765
162.744832	743.440905	4.911616	-0.030492	1.523701
163.203581	751.778706	4.916621	-0.030583	1.531637
163.571258	760.110851	4.921626	-0.030657	1.539513
164.891444	768.269937	4.926630	-0.030908	1.547331
165.501441	776.557575	4.931635	-0.031027	1.555122
165.882246	784.862772	4.936640	-0.031103	1.562856
166.950435	793.046832	4.941645	-0.031307	1.570543
167.401068	801.360543	4.946650	-0.031396	1.578219
168.235231	809.565798	4.951654	-0.031557	1.585815
169.176361	817.767788	4.956659	-0.031737	1.593387
170.131813	825.953199	4.961664	-0.031921	1.600911
170.832121	834.217063	4.966669	-0.032056	1.608432
170.989225	842.538946	4.971674	-0.032091	1.615892
171.612608	850.782156	4.976678	-0.032212	1.623314
172.286609	859.013351	4.981683	-0.032343	1.630699
173.313992	867.167911	4.986688	-0.032539	1.638033
173.810839	875.391902	4.991693	-0.032637	1.645320
174.055416	883.677298	4.996698	-0.032688	1.652593
174.466104	891.910271	5.001702	-0.032770	1.659812
175.181976	900.068497	5.006707	-0.032908	1.666976
176.038859	908.238593	5.011712	-0.033073	1.674140
176.566672	916.443918	5.016717	-0.033177	1.681257
176.960492	924.668387	5.021722	-0.033255	1.688343
178.214891	932.753317	5.026726	-0.033494	1.695397
178.904659	940.944563	5.031731	-0.033628	1.702435
179.525406	949.158792	5.036736	-0.033749	1.709454
180.086272	957.374154	5.041741	-0.033858	1.716437
181.092055	965.468681	5.046746	-0.034051	1.723349
182.147822	973.601485	5.051750	-0.034253	1.730272
183.119148	981.750209	5.056755	-0.034439	1.737169
183.669471	989.961236	5.061760	-0.034546	1.744035
184.017184	998.214990	5.066765	-0.034616	1.750883
185.172094	1006.289107	5.071770	-0.034837	1.757661
186.371462	1014.401068	5.076774	-0.035065	1.764449
187.209248	1022.574167	5.081779	-0.035226	1.771214
187.985790	1030.775073	5.086784	-0.035376	1.777968
188.911544	1038.931335	5.091789	-0.035554	1.784679
189.639003	1047.125064	5.096794	-0.035695	1.791370
190.032524	1055.374993	5.101798	-0.035773	1.798039
190.899674	1063.451980	5.106803	-0.035940	1.804604
191.863681	1071.596263	5.111808	-0.036124	1.811210
192.849265	1079.713130	5.116813	-0.036313	1.817773
193.495640	1087.865697	5.121818	-0.036439	1.824299
194.305156	1096.035615	5.126822	-0.036595	1.830835
194.772764	1104.241259	5.131827	-0.036687	1.837333
195.882603	1112.318347	5.136832	-0.036899	1.843786
197.354852	1120.370464	5.141837	-0.037178	1.850240
198.379368	1128.498347	5.146842	-0.037374	1.856676
198.799190	1136.741330	5.151846	-0.037458	1.863107
199.414986	1144.906777	5.156851	-0.037578	1.869479
200.107985	1153.061819	5.161856	-0.037712	1.875831
200.980790	1161.177488	5.166861	-0.037879	1.882152
201.531437	1169.326002	5.171866	-0.037987	1.888438
202.003457	1177.536166	5.176870	-0.038080	1.894742
202.916910	1185.617682	5.181875	-0.038256	1.900978
203.780095	1193.727194	5.186880	-0.038422	1.907208
204.401131	1201.915108	5.191885	-0.038542	1.913450
205.319105	1209.988733	5.196890	-0.038719	1.919619
205.751816	1218.198152	5.201894	-0.038804	1.925814
206.356031	1226.322797	5.206899	-0.038922	1.931946
207.026822	1234.441900	5.211904	-0.039052	1.938061
208.135519	1242.500761	5.216909	-0.039264	1.944161
208.245730	1250.732309	5.221914	-0.039290	1.950258
209.333426	1258.780960	5.226918	-0.039497	1.956310
209.703747	1266.941564	5.231923	-0.039571	1.962346
210.262336	1275.058831	5.236928	-0.039681	1.968353
210.953493	1283.171467	5.241933	-0.039815	1.974351
211.761581	1291.236698	5.246938	-0.039970	1.980310
212.432302	1299.379556	5.251942	-0.040100	1.986292
213.300886	1307.466169	5.256947	-0.040267	1.992237
214.003417	1315.599840	5.261952	-0.040403	1.998180
214.973453	1323.668096	5.266957	-0.040589	2.004086
215.967708	1331.729265	5.271962	-0.040779	2.009973
216.891198	1339.843571	5.276966	-0.040957	2.015872
217.617366	1347.960812	5.281971	-0.041097	2.021735
218.178700	1356.113667	5.286976	-0.041207	2.027589
218.938048	1364.253134	5.291981	-0.041353	2.033437
219.948673	1372.278047	5.296986	-0.041547	2.039214
221.042037	1380.331221	5.301990	-0.041755	2.045002
221.308241	1388.556837	5.306995	-0.041810	2.050809
222.417135	1396.604456	5.312000	-0.042022	2.056562
222.899437	1404.780962	5.317005	-0.042117	2.062324
223.562631	1412.896113	5.322010	-0.042246	2.068046
224.350466	1421.007040	5.327014	-0.042397	2.073762
225.660586	1428.973245	5.332019	-0.042646	2.079414
225.832972	1437.176759	5.337024	-0.042684	2.085100
226.134700	1445.361501	5.342029	-0.042745	2.090770
226.909210	1453.424346	5.347034	-0.042895	2.096389
227.506932	1461.543831	5.352038	-0.043011	2.102013
228.140001	1469.658237	5.357043	-0.043134	2.107623
228.672672	1477.785492	5.362048	-0.043239	2.113216
230.074132	1485.744264	5.367053	-0.043505	2.118765
230.313027	1493.898019	5.372058	-0.043554	2.124317
231.246817	1501.955133	5.377062	-0.043733	2.129858
232.006587	1510.030338	5.382067	-0.043880	2.135379
232.872913	1518.114482	5.387072	-0.044047	2.140902
233.130593	1526.305417	5.392077	-0.044100	2.146423
234.065315	1534.324652	5.397082	-0.044279	2.151881
234.829756	1542.438565	5.402086	-0.044427	2.157371
235.415928	1550.512444	5.407091	-0.044541	2.162803
236.087432	1558.607345	5.412096	-0.044671	2.168244
236.940141	1566.697451	5.417101	-0.044835	2.173685
237.215902	1574.842083	5.422106	-0.044892	2.179094
238.108783	1582.876814	5.427110	-0.045063	2.184474
238.282026	1591.067699	5.432115	-0.045100	2.189877
239.394780	1599.060419	5.437120	-0.045313	2.195224
239.863938	1607.167406	5.442125	-0.045405	2.200573
240.631424	1615.205048	5.447130	-0.045553	2.205890
241.307853	1623.322350	5.452134	-0.045685	2.211239
241.992415	1631.399248	5.457139	-0.045817	2.216548
242.381736	1639.539373	5.462144	-0.045895	2.221859
242.846562	1647.656486	5.467149	-0.045987	2.227149
243.408489	1655.733553	5.472154	-0.046096	2.232410
243.985490	1663.807573	5.477158	-0.046209	2.237657
244.709272	1671.854337	5.482163	-0.046349	2.242888
244.608477	1680.075962	5.487168	-0.046336	2.248144
245.244069	1688.131810	5.492173	-0.046459	2.253348
246.153677	1696.118213	5.497178	-0.046634	2.258520
246.947365	1704.169736	5.502182	-0.046786	2.263711
247.679620	1712.242969	5.507187	-0.046928	2.268898
248.021571	1720.406543	5.512192	-0.046997	2.274096
248.818316	1728.437793	5.517197	-0.047150	2.279238
249.385002	1736.465111	5.522202	-0.047261	2.284346
249.788640	1744.594041	5.527206	-0.047341	2.289492
250.686481	1752.611424	5.532211	-0.047514	2.294600
251.625056	1760.622463	5.537216	-0.047694	2.299695
251.717677	1768.823666	5.542221	-0.047716	2.304825
252.601116	1776.831484	5.547226	-0.047886	2.309891
253.400858	1784.919791	5.552230	-0.048040	2.314988
254.551963	1792.883282	5.557235	-0.048259	2.320027
255.405488	1800.912517	5.562240	-0.048423	2.325069
256.042053	1809.064638	5.567245	-0.048547	2.330158
256.799825	1817.130480	5.572250	-0.048693	2.335193
257.400581	1825.251459	5.577254	-0.048810	2.340238
258.000831	1833.314823	5.582259	-0.048927	2.345236
258.519913	1841.432383	5.587264	-0.049029	2.350250
258.933248	1849.545449	5.592269	-0.049111	2.355241
259.359296	1857.604070	5.597274	-0.049196	2.360190
260.405796	1865.603515	5.602278	-0.049396	2.365143
261.283861	1873.635013	5.607283	-0.049564	2.370092
261.594051	1881.770964	5.612288	-0.049627	2.375046
262.029811	1889.891675	5.617293	-0.049714	2.379991
263.459998	1897.812966	5.622298	-0.049985	2.384887
264.361607	1905.913724	5.627302	-0.050158	2.389837
264.998466	1913.996987	5.632307	-0.050282	2.394745
266.123583	1921.997892	5.637312	-0.050497	2.399633
267.288797	1930.002147	5.642317	-0.050719	2.404515
267.870996	1938.133106	5.647322	-0.050832	2.409417
268.339357	1946.258467	5.652326	-0.050925	2.414296
269.024095	1954.337313	5.657331	-0.051057	2.419155
269.519357	1962.433872	5.662336	-0.051155	2.423999
270.287557	1970.522023	5.667341	-0.051303	2.428850
271.244121	1978.550838	5.672346	-0.051486	2.433671
272.334328	1986.562870	5.677350	-0.051694	2.438482
273.011005	1994.616996	5.682355	-0.051826	2.443277
273.889017	2002.656001	5.687360	-0.051994	2.448068
275.088214	2010.689475	5.692365	-0.052223	2.452872
275.303212	2018.851824	5.697370	-0.052268	2.457666
275.513388	2027.014577	5.702374	-0.052312	2.462450
275.902490	2035.104983	5.707379	-0.052390	2.467196
276.706877	2043.108687	5.712384	-0.052545	2.471914
277.590966	2051.132841	5.717389	-0.052715	2.476641
278.052889	2059.211132	5.722394	-0.052806	2.481358
278.863374	2067.224206	5.727398	-0.052962	2.486055
279.756729	2075.280856	5.732403	-0.053133	2.490774
280.822911	2083.315689	5.737408	-0.053337	2.495484
280.865416	2091.516573	5.742413	-0.053350	2.500205
281.528545	2099.541676	5.747418	-0.053479	2.504861
282.096408	2107.659112	5.752422	-0.053590	2.509555
282.936399	2115.685334	5.757427	-0.053751	2.514208
283.535079	2123.703130	5.762432	-0.053868	2.518829
284.717162	2131.678604	5.767437	-0.054093	2.523460
285.668873	2139.716467	5.772442	-0.054275	2.528102
286.540010	2147.796038	5.777446	-0.054443	2.532752
287.391112	2155.828796	5.782451	-0.054606	2.537366
288.101709	2163.884787	5.787456	-0.054744	2.541974
289.033049	2171.941989	5.792461	-0.054923	2.546590
289.934838	2180.006539	5.797466	-0.055096	2.551200
290.893208	2188.058199	5.802470	-0.055279	2.555798
291.719192	2196.126531	5.807475	-0.055438	2.560387
292.759786	2204.122074	5.812480	-0.055637	2.564942
293.431374	2212.238000	5.817485	-0.055767	2.569531
294.205332	2220.312516	5.822490	-0.055917	2.574095
295.033246	2228.383532	5.827494	-0.056076	2.578652
295.264206	2236.513925	5.832499	-0.056124	2.583193
296.043500	2244.545973	5.837504	-0.056274	2.587709
297.125246	2252.640369	5.842509	-0.056481	2.592273
297.919470	2260.658300	5.847514	-0.056634	2.596766
298.803536	2268.689226	5.852518	-0.056804	2.601265
299.360166	2276.745080	5.857523	-0.056913	2.605747
300.088334	2284.788566	5.862528	-0.057053	2.610226
300.590317	2292.910981	5.867533	-0.057152	2.614725
301.360915	2300.898005	5.872538	-0.057301	2.619161
301.902567	2308.951534	5.877542	-0.057407	2.623609
302.925556	2316.939463	5.882547	-0.057602	2.628047
303.678287	2325.008580	5.887552	-0.057748	2.632503
304.692248	2333.045674	5.892557	-0.057942	2.636952
305.239718	2341.106486	5.897562	-0.058049	2.641374
305.929843	2349.165809	5.902566	-0.058182	2.645798
306.622220	2357.255191	5.907571	-0.058316	2.650230
308.041911	2365.203682	5.912576	-0.058586	2.654627
309.156322	2373.246852	5.917581	-0.058798	2.659048
309.429211	2381.373863	5.922586	-0.058855	2.663450
310.282188	2389.424785	5.927590	-0.059019	2.667842
310.739182	2397.541466	5.932595	-0.059109	2.672237
311.486220	2405.560662	5.937600	-0.059253	2.676590
311.773432	2413.682136	5.942605	-0.059312	2.680961
312.490806	2421.658343	5.947610	-0.059450	2.685276
313.112459	2429.722041	5.952614	-0.059571	2.689623
313.982799	2437.744937	5.957619	-0.059739	2.693958
314.977197	2445.765062	5.962624	-0.059929	2.698293
315.466813	2453.888001	5.967629	-0.060025	2.702642
315.964037	2461.948042	5.972634	-0.060123	2.706951
317.349416	2469.901679	5.977638	-0.060386	2.711254
318.026970	2477.974711	5.982643	-0.060517	2.715568
318.667574	2486.035849	5.987648	-0.060642	2.719866
319.966251	2494.022816	5.992653	-0.060889	2.724159
320.750381	2502.072959	5.997658	-0.061040	2.728447
321.720023	2510.115220	6.002662	-0.061226	2.732735
322.595874	2518.150338	6.007667	-0.061394	2.737006
323.158463	2526.262724	6.012672	-0.061504	2.741292
323.209075	2534.437755	6.017677	-0.061518	2.745572
323.453812	2542.524138	6.022682	-0.061569	2.749810
324.544643	2550.537715	6.027686	-0.061777	2.754057
325.245557	2558.553491	6.032691	-0.061913	2.758274
326.083730	2566.522438	6.037696	-0.062074	2.762468
326.761608	2574.577686	6.042701	-0.062206	2.766691
327.445283	2582.668468	6.047706	-0.062338	2.770926
328.543207	2590.646600	6.052710	-0.062548	2.775121
329.306898	2598.675500	6.057715	-0.062695	2.779316
330.670015	2606.627290	6.062720	-0.062954	2.783501
330.929518	2614.813859	6.067725	-0.063007	2.787733
331.942857	2622.789442	6.072730	-0.063201	2.791896
332.590766	2630.881604	6.077734	-0.063327	2.796091
333.576086	2638.898245	6.082739	-0.063516	2.800260
333.902309	2646.959504	6.087744	-0.063582	2.804407
335.517880	2654.886863	6.092749	-0.063887	2.808555
335.978878	2663.057390	6.097754	-0.063979	2.812753
336.724136	2671.098392	6.102758	-0.064122	2.816895
337.212639	2679.187454	6.107763	-0.064219	2.821041
337.907986	2687.229189	6.112768	-0.064353	2.825168
338.877670	2695.259511	6.117773	-0.064539	2.829299
339.596465	2703.301355	6.122778	-0.064678	2.833416
340.055070	2711.391943	6.127782	-0.064769	2.837535
341.264309	2719.333151	6.132787	-0.064999	2.841617
341.500095	2727.469581	6.137792	-0.065048	2.845735
342.489916	2735.450019	6.142797	-0.065237	2.849812
343.740971	2743.427593	6.147802	-0.065475	2.853896
344.660417	2751.477405	6.152806	-0.065652	2.857991
345.942124	2759.470132	6.157811	-0.065895	2.862073
346.622955	2767.564916	6.162816	-0.066027	2.866165
347.237928	2775.695976	6.167821	-0.066147	2.870266
347.858152	2783.696394	6.172826	-0.066268	2.874296
348.523697	2791.787241	6.177830	-0.066397	2.878367
349.494778	2799.785268	6.182835	-0.066583	2.882404
350.312628	2807.812262	6.187840	-0.066740	2.886441
350.966705	2815.930982	6.192845	-0.066867	2.890508
351.573347	2823.957173	6.197850	-0.066985	2.894521
352.266913	2831.999014	6.202854	-0.067120	2.898541
353.029566	2839.987831	6.207859	-0.067267	2.902533
353.339218	2848.090392	6.212864	-0.067330	2.906550
353.976296	2856.193299	6.217869	-0.067453	2.910580
354.183451	2864.298380	6.222874	-0.067497	2.914582
354.584768	2872.319510	6.227878	-0.067577	2.918548
355.567081	2880.229646	6.232883	-0.067765	2.922485
355.728664	2888.323747	6.237888	-0.067800	2.926462
356.178396	2896.389558	6.242893	-0.067889	2.930436
356.793400	2904.384507	6.247898	-0.068009	2.934378
357.299956	2912.428041	6.252902	-0.068108	2.938333
357.489356	2920.516160	6.257907	-0.068149	2.942288
358.166490	2928.544609	6.262912	-0.068280	2.946234
359.202209	2936.495587	6.267917	-0.068478	2.950155
359.668386	2944.526204	6.272922	-0.068570	2.954080
360.110032	2952.641924	6.277926	-0.068657	2.958040
360.812043	2960.621176	6.282931	-0.068793	2.961942
361.219118	2968.696255	6.287936	-0.068874	2.965869
361.703145	2976.746778	6.292941	-0.068969	2.969784
362.336333	2984.793379	6.297946	-0.069092	2.973699
363.561179	2992.721669	6.302950	-0.069326	2.977582
364.179912	3000.796303	6.307955	-0.069446	2.981499
364.578915	3008.857382	6.312960	-0.069525	2.985393
365.525846	3016.906279	6.317965	-0.069707	2.989305
366.527371	3024.873694	6.322970	-0.069899	2.993174
367.092779	3032.959237	6.327974	-0.070009	2.997073
368.061827	3040.946582	6.332979	-0.070195	3.000940
369.040572	3048.918197	6.337984	-0.070382	3.004795
369.657890	3057.022836	6.342989	-0.070502	3.008691
370.268263	3065.083279	6.347994	-0.070621	3.012559
371.498218	3073.101346	6.352998	-0.070855	3.016433
371.689873	3081.226214	6.358003	-0.070896	3.020301
372.142791	3089.257658	6.363008	-0.070985	3.024133
372.837987	3097.320213	6.368013	-0.071120	3.027986
373.231272	3105.375586	6.373018	-0.071198	3.031816
374.465551	3113.303622	6.378022	-0.071433	3.035623
375.268508	3121.319166	6.383027	-0.071588	3.039445
375.857946	3129.350286	6.388032	-0.071703	3.043258
376.326118	3137.462183	6.393037	-0.071795	3.047099
377.002267	3145.502456	6.398042	-0.071926	3.050911
377.275417	3153.622270	6.403046	-0.071982	3.054736
377.672035	3161.646336	6.408051	-0.072061	3.058518
378.278949	3169.639449	6.413056	-0.072179	3.062290
379.058492	3177.683033	6.418061	-0.072330	3.066089
379.547943	3185.703362	6.423066	-0.072426	3.069859
380.536372	3193.744774	6.428070	-0.072615	3.073658
380.821005	3201.802517	6.433075	-0.072673	3.077426
381.298182	3209.811631	6.438080	-0.072767	3.081176
381.793398	3217.846386	6.443085	-0.072865	3.084934
382.592886	3225.842655	6.448090	-0.073019	3.088684
383.523239	3233.867403	6.453094	-0.073197	3.092448
383.762521	3241.978062	6.458099	-0.073247	3.096215
384.170900	3250.009979	6.463104	-0.073328	3.099949
385.065153	3258.019506	6.468109	-0.073500	3.103691
385.494999	3266.025838	6.473114	-0.073585	3.107405
386.451068	3274.083810	6.478118	-0.073768	3.111162
387.236601	3282.070095	6.483123	-0.073919	3.114875
388.055485	3290.078597	6.488128	-0.074077	3.118594
388.559958	3298.155827	6.493133	-0.074176	3.122325
389.068425	3306.207165	6.498138	-0.074276	3.126041
390.136953	3314.193320	6.503142	-0.074480	3.129748
390.682661	3322.285994	6.508147	-0.074587	3.133475
391.328066	3330.315092	6.513152	-0.074712	3.137173
392.280866	3338.341281	6.518157	-0.074895	3.140879
392.749008	3346.379548	6.523162	-0.074987	3.144564
393.675215	3354.398664	6.528166	-0.075165	3.148257
394.665878	3362.400708	6.533171	-0.075354	3.151940
396.037830	3370.343439	6.538176	-0.075615	3.155609
395.873225	3378.547667	6.543181	-0.075589	3.159324
396.041257	3386.625439	6.548186	-0.075626	3.162991
397.268656	3394.595177	6.553190	-0.075859	3.166653
398.050237	3402.625232	6.558195	-0.076010	3.170318
398.999857	3410.587027	6.563200	-0.076192	3.173954
400.329688	3418.580324	6.568205	-0.076445	3.177618
400.236080	3426.739762	6.573210	-0.076433	3.181289
400.872340	3434.776771	6.578214	-0.076556	3.184933
401.852669	3442.737219	6.583219	-0.076744	3.188553
402.760483	3450.749700	6.588224	-0.076918	3.192190
403.058871	3458.874361	6.593229	-0.076979	3.195846
403.627782	3466.872285	6.598234	-0.077090	3.199452
404.282868	3474.912458	6.603238	-0.077217	3.203077
404.945705	3482.945954	6.608243	-0.077346	3.206695
405.758769	3490.955618	6.613248	-0.077502	3.210305
406.305123	3499.058289	6.618253	-0.077609	3.213940
406.806098	3507.064602	6.623258	-0.077707	3.217527
407.850352	3515.062248	6.628262	-0.077907	3.221128
408.520959	3523.076643	6.633267	-0.078037	3.224717
408.952381	3531.156701	6.638272	-0.078122	3.228322
409.567346	3539.215311	6.643277	-0.078242	3.231920
410.231607	3547.193921	6.648282	-0.078371	3.235480
410.889965	3555.212580	6.653286	-0.078499	3.239054
411.441343	3563.241972	6.658291	-0.078606	3.242625
412.351482	3571.218627	6.663296	-0.078781	3.246183
412.385142	3579.379123	6.668301	-0.078793	3.249781
412.922175	3587.390432	6.673306	-0.078898	3.253331
413.555779	3595.415282	6.678310	-0.079021	3.256887
414.563407	3603.413112	6.683315	-0.079214	3.260442
415.584563	3611.363410	6.688320	-0.079409	3.263972
415.948349	3619.501101	6.693325	-0.079482	3.267554
416.325562	3627.597452	6.698330	-0.079557	3.271115
416.875192	3635.624838	6.703334	-0.079665	3.274649
417.673524	3643.569724	6.708339	-0.079818	3.278152
418.278980	3651.597703	6.713344	-0.079936	3.281680
419.183327	3659.605172	6.718349	-0.080110	3.285208
420.002245	3667.596494	6.723354	-0.080267	3.288720
420.741037	3675.680886	6.728358	-0.080410	3.292267
420.928013	3683.817980	6.733363	-0.080450	3.295810
421.759859	3691.745784	6.738368	-0.080610	3.299284
422.861305	3699.758122	6.743373	-0.080820	3.302802
423.051074	3707.830744	6.748378	-0.080861	3.306306
423.891510	3715.841939	6.753382	-0.081022	3.309805
424.268438	3723.944832	6.758387	-0.081098	3.313322
425.462349	3731.856743	6.763392	-0.081325	3.316784
426.398883	3739.889592	6.768397	-0.081505	3.320285
426.631545	3747.930351	6.773402	-0.081553	3.323758
427.556748	3755.929632	6.778406	-0.081731	3.327237
428.562639	3763.959640	6.783411	-0.081923	3.330727
428.751608	3772.081117	6.788416	-0.081963	3.334222
429.923050	3780.050116	6.793421	-0.082187	3.337686
430.413804	3788.102571	6.798426	-0.082283	3.341155
431.413188	3796.090434	6.803430	-0.082474	3.344612
431.717318	3804.213825	6.808435	-0.082536	3.348098
432.430989	3812.207600	6.813440	-0.082674	3.351539
433.108713	3820.276764	6.818445	-0.082806	3.355008
433.348411	3828.321002	6.823450	-0.082855	3.358447
434.064664	3836.302809	6.828454	-0.082994	3.361872
435.451251	3844.203354	6.833459	-0.083257	3.365285
435.153336	3852.418698	6.838464	-0.083207	3.368765
435.975868	3860.440379	6.843469	-0.083365	3.372201
436.782714	3868.422650	6.848474	-0.083521	3.375616
437.604641	3876.422424	6.853478	-0.083679	3.379035
438.524756	3884.438515	6.858483	-0.083855	3.382461
438.723305	3892.524956	6.863488	-0.083897	3.385887
439.359482	3900.555687	6.868493	-0.084021	3.389302
439.980370	3908.643513	6.873498	-0.084142	3.392737
440.714065	3916.627243	6.878502	-0.084284	3.396128
441.464482	3924.608990	6.883507	-0.084428	3.399516
441.613608	3932.676678	6.888512	-0.084461	3.402915
442.078730	3940.746646	6.893517	-0.084553	3.406323
442.608789	3948.721981	6.898522	-0.084657	3.409689
443.467344	3956.728502	6.903526	-0.084822	3.413077
444.178425	3964.781107	6.908531	-0.084959	3.416476
444.702779	3972.769629	6.913536	-0.085062	3.419838
445.277135	3980.858466	6.918541	-0.085174	3.423240
446.459424	3988.789865	6.923546	-0.085400	3.426594
447.161837	3996.863772	6.928550	-0.085535	3.429987
447.720888	4004.879214	6.933555	-0.085645	3.433348
448.314589	4012.905168	6.938560	-0.085760	3.436710
449.029971	4020.971285	6.943565	-0.085899	3.440090
449.644789	4028.966773	6.948570	-0.086018	3.443434
449.966927	4037.050015	6.953574	-0.086084	3.446801
450.780851	4045.061157	6.958579	-0.086240	3.450152
451.446506	4053.038311	6.963584	-0.086369	3.453480
452.117750	4061.065279	6.968589	-0.086499	3.456826
452.515180	4069.133926	6.973594	-0.086579	3.460176
453.145437	4077.119894	6.978598	-0.086701	3.463496
453.461887	4085.226230	6.983603	-0.086765	3.466853
454.233373	4093.221307	6.988608	-0.086914	3.470175
454.787644	4101.285115	6.993613	-0.087022	3.473516
455.081735	4109.312566	6.998618	-0.087082	3.476829
455.708817	4117.292286	7.003622	-0.087204	3.480130
456.926346	4125.215232	7.008627	-0.087436	3.483425
457.210476	4133.349265	7.013632	-0.087494	3.486772
457.867179	4141.399167	7.018637	-0.087621	3.490093
458.584467	4149.369884	7.023642	-0.087760	3.493381
459.569102	4157.379983	7.028646	-0.087949	3.496690
459.975495	4165.433056	7.033651	-0.088029	3.499995
460.529839	4173.460880	7.038656	-0.088138	3.503292
461.353749	4181.492982	7.043661	-0.088296	3.506595
461.832031	4189.515664	7.048666	-0.088391	3.509880
461.933608	4197.650681	7.053670	-0.088415	3.513196
462.795117	4205.629058	7.058675	-0.088580	3.516469
463.260163	4213.616109	7.063680	-0.088672	3.519730
463.813639	4221.652397	7.068685	-0.088780	3.523011
464.861335	4229.609729	7.073690	-0.088980	3.526272
465.348113	4237.705258	7.078694	-0.089076	3.529568
465.919623	4245.738817	7.083699	-0.089188	3.532839
466.713377	4253.749147	7.088704	-0.089341	3.536104
467.141011	4261.796041	7.093709	-0.089425	3.539369
467.855244	4269.771454	7.098714	-0.089563	3.542611
468.468888	4277.803206	7.103718	-0.089683	3.545870
469.062610	4285.882902	7.108723	-0.089799	3.549144
469.448523	4293.948842	7.113728	-0.089876	3.552404
470.239365	4301.982477	7.118733	-0.090028	3.555659
470.442755	4309.950741	7.123738	-0.090071	3.558868
471.237170	4317.966684	7.128742	-0.090224	3.562110
471.787952	4325.949384	7.133747	-0.090332	3.565329
472.171711	4334.001919	7.138752	-0.090408	3.568568
472.861031	4342.074280	7.143757	-0.090542	3.571821
474.026306	4349.956543	7.148762	-0.090764	3.575008
474.995016	4357.980525	7.153766	-0.090949	3.578244
475.616278	4366.051212	7.158771	-0.091070	3.581485
476.287037	4374.037382	7.163776	-0.091200	3.584691
477.341628	4382.075668	7.168781	-0.091402	3.587925
477.707741	4390.184748	7.173786	-0.091475	3.591165
478.687868	4398.135510	7.178790	-0.091663	3.594357
479.297304	4406.216704	7.183795	-0.091781	3.597586
479.337507	4414.296521	7.188800	-0.091794	3.600796
480.922199	4422.154219	7.193805	-0.092094	3.603959
481.128220	4430.298955	7.198810	-0.092138	3.607194
481.983541	4438.323811	7.203814	-0.092302	3.610396
482.075094	4446.433249	7.208819	-0.092324	3.613608
482.693816	4454.421262	7.213824	-0.092445	3.616783
482.980209	4462.477533	7.218829	-0.092503	3.619973
483.340451	4470.452670	7.223834	-0.092575	3.623130
484.131388	4478.504099	7.228838	-0.092728	3.626327
484.733570	4486.531994	7.233843	-0.092845	3.629506
485.496378	4494.476479	7.238848	-0.092992	3.632654
486.350916	4502.530557	7.243853	-0.093157	3.635845
486.627989	4510.569939	7.248858	-0.093213	3.639011
487.015772	4518.640515	7.253862	-0.093291	3.642189
487.224355	4526.667150	7.258867	-0.093335	3.645343
487.847192	4534.632071	7.263872	-0.093456	3.648481
488.567010	4542.703501	7.268877	-0.093595	3.651660
489.445106	4550.643552	7.273882	-0.093763	3.654790
490.359251	4558.643465	7.278886	-0.093939	3.657941
490.682645	4566.757050	7.283891	-0.094004	3.661117
490.858442	4574.704644	7.288896	-0.094042	3.664222
492.093346	4582.723438	7.293901	-0.094277	3.667381
492.897713	4590.755101	7.298906	-0.094432	3.670530
493.857240	4598.723247	7.303910	-0.094616	3.673656
494.357782	4606.808568	7.308915	-0.094714	3.676812
494.409207	4614.885685	7.313920	-0.094729	3.679951
494.971438	4622.920708	7.318925	-0.094839	3.683084
495.512108	4630.948176	7.323930	-0.094945	3.686210
496.257515	4638.939119	7.328934	-0.095089	3.689326
496.653976	4647.045269	7.333939	-0.095168	3.692473
497.023655	4655.078743	7.338944	-0.095242	3.695590
497.522192	4663.092804	7.343949	-0.095339	3.698699
498.179571	4671.069311	7.348954	-0.095467	3.701796
498.493837	4679.081188	7.353958	-0.095531	3.704894
499.669419	4687.027653	7.358963	-0.095755	3.707987
500.201608	4695.142867	7.363968	-0.095859	3.711126
500.614551	4703.210519	7.368973	-0.095941	3.714240
501.131463	4711.199524	7.373978	-0.096042	3.717324
502.023290	4719.153868	7.378982	-0.096213	3.720402
502.876664	4727.151072	7.383987	-0.096378	3.723492
503.271553	4735.197254	7.388992	-0.096456	3.726588
503.950424	4743.275975	7.393997	-0.096588	3.729700
504.099881	4751.383631	7.399002	-0.096621	3.732807
504.688888	4759.373523	7.404006	-0.096736	3.735877
505.170796	4767.363223	7.409011	-0.096830	3.738943
506.008224	4775.320641	7.414016	-0.096991	3.742002
506.379392	4783.377662	7.419021	-0.097066	3.745085
506.971841	4791.356993	7.424026	-0.097181	3.748141
507.612060	4799.445864	7.429030	-0.097306	3.751237
508.172669	4807.435119	7.434035	-0.097415	3.754291
508.801514	4815.435059	7.439040	-0.097537	3.757348
509.438622	4823.499649	7.444045	-0.097661	3.760427
509.856214	4831.511628	7.449050	-0.097744	3.763479
510.323898	4839.583175	7.454054	-0.097836	3.766551
510.945871	4847.570367	7.459059	-0.097957	3.769593
511.541184	4855.599757	7.464064	-0.098073	3.772648
512.524103	4863.591385	7.469069	-0.098261	3.775694
512.826398	4871.625144	7.474074	-0.098323	3.778739
513.784972	4879.611250	7.479078	-0.098506	3.781778
514.296238	4887.671253	7.484083	-0.098607	3.784832
514.905486	4895.686486	7.489088	-0.098725	3.787868
515.608142	4903.750832	7.494093	-0.098861	3.790923
516.455800	4911.704564	7.499098	-0.099024	3.793937
517.046250	4919.746094	7.504102	-0.099139	3.796976
517.264270	4927.815881	7.509107	-0.099185	3.800014
518.218103	4935.719270	7.514112	-0.099368	3.803004
519.416179	4943.751212	7.519117	-0.099596	3.806045
519.310847	4951.869325	7.524122	-0.099582	3.809087
519.492966	4959.941832	7.529126	-0.099621	3.812116
520.865637	4967.866229	7.534131	-0.099881	3.815113
521.240197	4975.897167	7.539136	-0.099956	3.818125
522.260723	4983.937645	7.544141	-0.100151	3.821153
522.665416	4991.922305	7.549146	-0.100232	3.824144
523.306183	4999.974123	7.554150	-0.100356	3.827163
524.173895	5007.991761	7.559155	-0.100523	3.830171
524.742732	5016.010764	7.564160	-0.100634	3.833171
525.679928	5024.026793	7.569165	-0.100814	3.836175
525.946443	5032.058710	7.574170	-0.100868	3.839169
527.171600	5040.032834	7.579174	-0.101102	3.842158
527.819940	5048.061795	7.584179	-0.101228	3.845154
528.581406	5056.105180	7.589184	-0.101375	3.848155
529.012038	5064.238807	7.594189	-0.101460	3.851180
529.685727	5072.211022	7.599194	-0.101590	3.854148
530.013611	5080.284242	7.604198	-0.101657	3.857143
530.622926	5088.310101	7.609203	-0.101775	3.860125
531.061379	5096.290310	7.614208	-0.101862	3.863083
532.051123	5104.307845	7.619213	-0.102051	3.866065
532.465821	5112.323317	7.624218	-0.102134	3.869031
533.179139	5120.395517	7.629222	-0.102272	3.872023
533.207179	5128.567155	7.634227	-0.102282	3.875034
534.124308	5136.418088	7.639232	-0.102458	3.877943
534.906421	5144.415993	7.644237	-0.102609	3.880901
535.960601	5152.346886	7.649242	-0.102810	3.883838
536.201148	5160.462802	7.654246	-0.102860	3.886824
536.669638	5168.468915	7.659251	-0.102953	3.889772
537.513609	5176.443173	7.664256	-0.103115	3.892713
538.394250	5184.434649	7.669261	-0.103284	3.895659
538.563733	5192.524378	7.674266	-0.103321	3.898624
538.813778	5200.561420	7.679270	-0.103372	3.901570
539.498579	5208.547373	7.684275	-0.103505	3.904503
540.046295	5216.582800	7.689280	-0.103612	3.907449
540.548623	5224.651741	7.694285	-0.103711	3.910405
541.432371	5232.608502	7.699290	-0.103880	3.913324
542.089765	5240.655422	7.704294	-0.104008	3.916270
542.902761	5248.617397	7.709299	-0.104165	3.919185
543.250007	5256.652768	7.714304	-0.104234	3.922116
544.368128	5264.638944	7.719309	-0.104448	3.925041
544.836256	5272.718375	7.724314	-0.104540	3.927986
545.137841	5280.820375	7.729318	-0.104601	3.930933
546.068100	5288.797435	7.734323	-0.104780	3.933845
546.768337	5296.819243	7.739328	-0.104915	3.936766
546.846774	5304.873716	7.744333	-0.104935	3.939685
547.727784	5312.849614	7.749338	-0.105104	3.942589
548.791922	5320.794923	7.754342	-0.105307	3.945482
549.478829	5328.882970	7.759347	-0.105440	3.948418
549.959391	5336.927990	7.764352	-0.105535	3.951333
551.260877	5344.890705	7.769357	-0.105782	3.954230
551.929864	5352.918899	7.774362	-0.105912	3.957137
552.836894	5360.900805	7.779366	-0.106086	3.960030
553.482035	5368.975546	7.784371	-0.106211	3.962949
553.772373	5377.012280	7.789376	-0.106271	3.965846
554.278088	5385.056675	7.794381	-0.106370	3.968747
554.726851	5393.129941	7.799386	-0.106459	3.971655
555.644856	5401.104848	7.804390	-0.106635	3.974535
556.672302	5409.069347	7.809395	-0.106831	3.977410
556.987478	5417.090791	7.814400	-0.106895	3.980291
557.902971	5425.094729	7.819405	-0.107071	3.983173
558.871339	5433.126780	7.824410	-0.107256	3.986065
558.909650	5441.193449	7.829414	-0.107268	3.988951
559.779134	5449.198793	7.834419	-0.107435	3.991827
560.512456	5457.184335	7.839424	-0.107577	3.994691
561.412795	5465.221493	7.844429	-0.107750	3.997575
562.635415	5473.171890	7.849434	-0.107983	4.000431
563.485194	5481.133527	7.854438	-0.108146	4.003282
563.652997	5489.329173	7.859443	-0.108182	4.006203
564.456696	5497.237449	7.864448	-0.108337	4.009030
565.223422	5505.365021	7.869453	-0.108485	4.011933
565.633734	5513.376195	7.874458	-0.108567	4.014786
566.069623	5521.414957	7.879462	-0.108653	4.017648
566.548738	5529.439204	7.884467	-0.108747	4.020502
567.651637	5537.358485	7.889472	-0.108958	4.023328
568.819588	5545.419292	7.894477	-0.109180	4.026202
569.327645	5553.393186	7.899482	-0.109280	4.029033
569.638811	5561.557331	7.904486	-0.109343	4.031926
570.776642	5569.555767	7.909491	-0.109560	4.034772
571.302036	5577.531599	7.914496	-0.109663	4.037597
571.842750	5585.606356	7.919501	-0.109769	4.040456
572.344472	5593.548884	7.924506	-0.109868	4.043266
573.033686	5601.546602	7.929510	-0.110001	4.046096
573.388481	5609.625849	7.934515	-0.110072	4.048947
574.143584	5617.645815	7.939520	-0.110218	4.051781
574.934111	5625.664880	7.944525	-0.110370	4.054614
575.015244	5633.742349	7.949530	-0.110391	4.057454
575.766706	5641.725055	7.954534	-0.110536	4.060269
576.820107	5649.699096	7.959539	-0.110737	4.063084
577.561603	5657.639693	7.964544	-0.110880	4.065880
578.691430	5665.694579	7.969549	-0.111096	4.068720
579.146758	5673.793471	7.974554	-0.111186	4.071563
579.490751	5681.785051	7.979558	-0.111255	4.074365
579.848719	5689.871002	7.984563	-0.111327	4.077198
580.629523	5697.808666	7.989568	-0.111477	4.079984
581.435503	5705.813654	7.994573	-0.111632	4.082791
581.969020	5713.908952	7.999578	-0.111737	4.085624
582.686488	5721.888041	8.004582	-0.111875	4.088417
583.540111	5729.948961	8.009587	-0.112040	4.091238
584.186615	5737.888701	8.014592	-0.112165	4.094012
585.039479	5746.001766	8.019597	-0.112329	4.096848
585.985183	5753.922273	8.024602	-0.112510	4.099615
587.226044	5761.900696	8.029606	-0.112746	4.102405
587.837749	5769.977219	8.034611	-0.112865	4.105218
588.791064	5777.968818	8.039616	-0.113048	4.108005
589.472686	5786.039844	8.044621	-0.113180	4.110813
590.098472	5794.030528	8.049626	-0.113302	4.113591
590.674432	5802.080200	8.054630	-0.113414	4.116386
591.614348	5810.067527	8.059635	-0.113594	4.119163
592.774583	5818.042330	8.064640	-0.113815	4.121936
592.977402	5826.128820	8.069645	-0.113858	4.124733
593.933374	5834.154554	8.074650	-0.114042	4.127518
594.605151	5842.194046	8.079654	-0.114172	4.130301
595.522775	5850.202926	8.084659	-0.114348	4.133075
596.770569	5858.161848	8.089664	-0.114585	4.135834
597.999013	5866.169951	8.094669	-0.114819	4.138607
599.004358	5874.221166	8.099674	-0.115011	4.141391
599.630297	5882.213055	8.104678	-0.115133	4.144147
600.970729	5890.246426	8.109683	-0.115388	4.146925
602.042090	5898.239077	8.114688	-0.115592	4.149683
603.004335	5906.328772	8.119693	-0.115777	4.152472
603.512739	5914.383128	8.124698	-0.115877	4.155240
604.385397	5922.349976	8.129702	-0.116044	4.157981
605.393018	5930.379701	8.134707	-0.116237	4.160744
606.442722	5938.302396	8.139712	-0.116438	4.163468
607.214143	5946.480567	8.144717	-0.116586	4.166274
607.987801	5954.438817	8.149722	-0.116736	4.169003
608.382629	5962.532696	8.154726	-0.116814	4.171773
609.645845	5970.516380	8.159731	-0.117055	4.174513
610.734548	5978.509040	8.164736	-0.117262	4.177251
611.622871	5986.536180	8.169741	-0.117433	4.179998
612.622145	5994.525820	8.174746	-0.117624	4.182731
613.425558	6002.560690	8.179750	-0.117779	4.185475
614.750441	6010.530591	8.184755	-0.118031	4.188201
615.427301	6018.629635	8.189760	-0.118162	4.190962
616.410296	6026.689323	8.194765	-0.118350	4.193711
617.053153	6034.742823	8.199770	-0.118475	4.196452
617.186278	6042.771451	8.204774	-0.118505	4.199177
618.082425	6050.793649	8.209779	-0.118677	4.201907
619.269328	6058.619472	8.214784	-0.118903	4.204571
620.270763	6066.679880	8.219789	-0.119095	4.207311
621.006010	6074.744240	8.224794	-0.119237	4.210048
621.994317	6082.768334	8.229798	-0.119426	4.212771
623.175768	6090.774444	8.234803	-0.119651	4.215489
624.093688	6098.728735	8.239808	-0.119827	4.218184
625.028620	6106.852716	8.244813	-0.120006	4.220935
625.766630	6114.816171	8.249818	-0.120149	4.223629
626.454241	6122.912591	8.254822	-0.120282	4.226364
628.040427	6130.837145	8.259827	-0.120582	4.229049
629.413352	6138.853614	8.264832	-0.120843	4.231761
630.152640	6146.930927	8.269837	-0.120986	4.234485
631.951270	6154.847626	8.274842	-0.121326	4.237163
632.939952	6162.854368	8.279846	-0.121515	4.239862
634.116651	6170.960695	8.284851	-0.121740	4.242595
634.645676	6179.006819	8.289856	-0.121843	4.245299
635.728177	6186.990169	8.294861	-0.122050	4.247985
636.757592	6194.990802	8.299866	-0.122247	4.250675
637.480356	6203.058831	8.304870	-0.122386	4.253383
638.987271	6211.056964	8.309875	-0.122672	4.256073
640.146686	6219.041570	8.314880	-0.122893	4.258753
641.425342	6227.090072	8.319885	-0.123136	4.261454
642.734063	6234.991855	8.324890	-0.123385	4.264104
644.591482	6242.998251	8.329894	-0.123736	4.266792
645.525387	6251.131149	8.334899	-0.123915	4.269513
646.631052	6259.113155	8.339904	-0.124126	4.272182
647.818438	6267.115309	8.344909	-0.124352	4.274857
648.521475	6275.250357	8.349914	-0.124489	4.277571
649.451758	6283.220528	8.354918	-0.124667	4.280230
650.312357	6291.249553	8.359923	-0.124832	4.282905
651.594143	6299.226934	8.364928	-0.125076	4.285566
652.941920	6307.197755	8.369933	-0.125332	4.288223
653.949266	6315.276013	8.374938	-0.125525	4.290911
655.052700	6323.251799	8.379942	-0.125735	4.293564
655.982592	6331.348599	8.384947	-0.125914	4.296254
656.643415	6339.284012	8.389952	-0.126042	4.298887
657.970235	6347.374189	8.394957	-0.126294	4.301574
658.422037	6355.387601	8.399962	-0.126383	4.304227
659.357996	6363.442541	8.404966	-0.126563	4.306896
661.185619	6371.339429	8.409971	-0.126908	4.309518
661.927963	6379.411777	8.414976	-0.127052	4.312188
662.993728	6387.416402	8.419981	-0.127255	4.314836
663.532061	6395.512747	8.424986	-0.127361	4.317508
664.391474	6403.491145	8.429990	-0.127526	4.320143
665.310877	6411.500895	8.434995	-0.127702	4.322786
666.704738	6419.374002	8.440000	-0.127967	4.325386
667.030495	6427.576023	8.445005	-0.128033	4.328085
668.344612	6435.552792	8.450010	-0.128282	4.330715
668.816927	6443.573779	8.455014	-0.128375	4.333352
669.842995	6451.647530	8.460019	-0.128572	4.336009
670.600236	6459.610661	8.465024	-0.128718	4.338625
671.550502	6467.649998	8.470029	-0.128900	4.341267
672.174744	6475.617746	8.475034	-0.129021	4.343880
673.112603	6483.668771	8.480038	-0.129201	4.346522
674.425279	6491.608295	8.485043	-0.129450	4.349128
674.809091	6499.705421	8.490048	-0.129527	4.351777
676.129970	6507.711686	8.495053	-0.129778	4.354401
677.327377	6515.724916	8.500058	-0.130006	4.357025
677.508348	6523.766108	8.505062	-0.130045	4.359650
678.735434	6531.772910	8.510067	-0.130279	4.362269
679.760121	6539.687486	8.515072	-0.130475	4.364855
680.455220	6547.815089	8.520077	-0.130609	4.367506
681.614800	6555.752664	8.525082	-0.130830	4.370096
682.565935	6563.783005	8.530086	-0.131012	4.372714
683.432068	6571.862461	8.535091	-0.131179	4.375346
683.955331	6579.863279	8.540096	-0.131281	4.377948
684.682255	6587.910464	8.545101	-0.131422	4.380565
685.789466	6595.899869	8.550106	-0.131633	4.383164
686.758104	6603.884499	8.555110	-0.131819	4.385758
687.390242	6612.006630	8.560115	-0.131942	4.388394
688.429635	6619.985791	8.565120	-0.132140	4.390984
689.306625	6628.017368	8.570125	-0.132309	4.393588
690.643632	6636.041161	8.575130	-0.132563	4.396191
691.033643	6644.074159	8.580135	-0.132641	4.398790
691.947214	6652.163016	8.585139	-0.132816	4.401408
692.962058	6660.015453	8.590144	-0.133010	4.403949
694.046334	6668.150433	8.595149	-0.133217	4.406579
694.911210	6676.184921	8.600154	-0.133383	4.409174
696.028039	6684.166107	8.605159	-0.133596	4.411752
696.928672	6692.179190	8.610163	-0.133769	4.414338
697.150401	6700.312007	8.615168	-0.133816	4.416956
698.346444	6708.250886	8.620173	-0.134043	4.419516
698.951955	6716.315772	8.625178	-0.134161	4.422112
699.751700	6724.231023	8.630183	-0.134315	4.424659
701.021199	6732.290902	8.635187	-0.134557	4.427253
701.507605	6740.327855	8.640192	-0.134653	4.429834
701.916162	6748.391300	8.645197	-0.134734	4.432422
702.993435	6756.311519	8.650202	-0.134939	4.434965
703.960091	6764.293889	8.655207	-0.135125	4.437527
705.251480	6772.297153	8.660211	-0.135370	4.440094
705.966970	6780.317531	8.665216	-0.135508	4.442664
706.108226	6788.463081	8.670221	-0.135540	4.445269
706.897567	6796.431692	8.675226	-0.135692	4.447818
708.153373	6804.406786	8.680231	-0.135931	4.450371
708.758874	6812.489472	8.685235	-0.136049	4.452953
709.192044	6820.466745	8.690240	-0.136135	4.455499
709.662716	6828.508041	8.695245	-0.136228	4.458064
710.202237	6836.534675	8.700250	-0.136333	4.460624
711.167819	6844.479463	8.705255	-0.136518	4.463157
712.140630	6852.514451	8.710259	-0.136704	4.465718
712.528416	6860.524144	8.715264	-0.136782	4.468267
713.404666	6868.602579	8.720269	-0.136950	4.470838
713.493815	6876.620423	8.725274	-0.136972	4.473385
714.420674	6884.625475	8.730279	-0.137149	4.475930
715.530644	6892.590108	8.735283	-0.137361	4.478461
716.313134	6900.659810	8.740288	-0.137512	4.481022
716.809820	6908.634064	8.745293	-0.137610	4.483551
717.564776	6916.681284	8.750298	-0.137755	4.486102
718.650280	6924.645119	8.755303	-0.137963	4.488627
719.725573	6932.711713	8.760307	-0.138168	4.491182
719.867058	6940.686974	8.765312	-0.138199	4.493704
720.773297	6948.760103	8.770317	-0.138373	4.496258
721.662622	6956.725624	8.775322	-0.138544	4.498776
722.207018	6964.781332	8.780327	-0.138651	4.501320
723.092316	6972.744639	8.785331	-0.138821	4.503835
723.749258	6980.800992	8.790336	-0.138948	4.506376
724.744681	6988.782869	8.795341	-0.139138	4.508894
725.587250	6996.873078	8.800346	-0.139301	4.511444
726.436003	7004.783582	8.805351	-0.139464	4.513935
727.090527	7012.887059	8.810355	-0.139591	4.516486
727.383851	7020.849246	8.815360	-0.139650	4.518989
727.820991	7028.979865	8.820365	-0.139737	4.521545
729.016478	7036.793220	8.825370	-0.139965	4.524001
729.622722	7044.918194	8.830375	-0.140083	4.526552
731.176417	7052.829094	8.835379	-0.140377	4.529036
731.987031	7060.947436	8.840384	-0.140533	4.531583
732.594900	7068.952420	8.845389	-0.140652	4.534091
732.978315	7077.073291	8.850394	-0.140728	4.536635
733.965574	7084.917559	8.855399	-0.140917	4.539091
734.851022	7093.032741	8.860403	-0.141087	4.541630
735.696519	7100.900264	8.865408	-0.141250	4.544091
736.875060	7109.019414	8.870413	-0.141474	4.546629
737.459432	7117.075873	8.875418	-0.141588	4.549145
737.321182	7125.152935	8.880423	-0.141568	4.551665
738.903705	7133.016187	8.885427	-0.141867	4.554119
739.539168	7141.116508	8.890432	-0.141991	4.556645
739.761332	7149.125303	8.895437	-0.142037	4.559140
740.750236	7157.143089	8.900442	-0.142227	4.561637
741.327139	7165.073122	8.905447	-0.142339	4.564105
742.514812	7173.202979	8.910451	-0.142565	4.566634
743.269194	7181.144601	8.915456	-0.142711	4.569103
744.288005	7189.240647	8.920461	-0.142906	4.571619
745.332775	7197.210688	8.925466	-0.143106	4.574094
746.150576	7205.236566	8.930471	-0.143263	4.576585
747.165122	7213.219186	8.935475	-0.143457	4.579061
748.021660	7221.285614	8.940480	-0.143622	4.581561
748.853919	7229.207630	8.945485	-0.143782	4.584015
750.061341	7237.293677	8.950490	-0.144012	4.586519
750.637408	7245.268024	8.955495	-0.144124	4.588987
751.143742	7253.419767	8.960499	-0.144224	4.591507
751.637054	7261.295276	8.965504	-0.144320	4.593941
752.781429	7269.370167	8.970509	-0.144539	4.596436
753.307429	7277.322395	8.975514	-0.144642	4.598890
754.083916	7285.370858	8.980519	-0.144791	4.601374
755.039403	7293.325526	8.985523	-0.144974	4.603827
755.767976	7301.395506	8.990528	-0.145115	4.606314
756.328209	7309.417550	8.995533	-0.145225	4.608784
757.225568	7317.437843	9.000538	-0.145397	4.611253
757.712502	7325.443667	9.005543	-0.145493	4.613716
758.287399	7333.557551	9.010547	-0.145605	4.616211
759.034949	7341.490093	9.015552	-0.145749	4.618649
760.174956	7349.510589	9.020557	-0.145967	4.621112
760.170457	7357.562814	9.025562	-0.145971	4.623584
760.647034	7365.518876	9.030567	-0.146065	4.626024
761.729652	7373.528712	9.035571	-0.146272	4.628480
762.502581	7381.575534	9.040576	-0.146421	4.630946
763.285812	7389.538266	9.045581	-0.146572	4.633385
763.753822	7397.591774	9.050586	-0.146664	4.635850
765.083268	7405.515399	9.055591	-0.146917	4.638273
765.965185	7413.651226	9.060595	-0.147086	4.640761
766.235809	7421.616832	9.065600	-0.147141	4.643195
767.286337	7429.633442	9.070605	-0.147342	4.645643
767.845643	7437.665793	9.075610	-0.147451	4.648094
768.069123	7445.777473	9.080615	-0.147498	4.650569
768.898205	7453.799013	9.085619	-0.147658	4.653015
770.027172	7461.755313	9.090624	-0.147873	4.655439
770.565668	7469.790176	9.095629	-0.147979	4.657886
771.589228	7477.787034	9.100634	-0.148174	4.660319
772.218824	7485.781926	9.105639	-0.148297	4.662751
772.676633	7493.890464	9.110643	-0.148387	4.665217
772.978346	7501.866210	9.115648	-0.148448	4.667641
773.286486	7509.936711	9.120653	-0.148511	4.670092
774.449981	7517.938218	9.125658	-0.148733	4.672520
774.926062	7526.006013	9.130663	-0.148826	4.674968
775.845258	7534.029913	9.135667	-0.149003	4.677400
776.424913	7541.937158	9.140672	-0.149116	4.679796
777.530928	7549.939040	9.145677	-0.149327	4.682219
778.433337	7557.923782	9.150682	-0.149500	4.684635
779.467277	7565.918905	9.155687	-0.149698	4.687053
780.886521	7573.905326	9.160691	-0.149967	4.689467
781.190610	7581.980619	9.165696	-0.150029	4.691907
781.595156	7590.067069	9.170701	-0.150109	4.694350
782.450315	7598.063587	9.175706	-0.150274	4.696763
783.026105	7606.012017	9.180711	-0.150386	4.699161
783.896036	7614.099242	9.185715	-0.150553	4.701599
784.079451	7622.041202	9.190720	-0.150592	4.703994
784.937034	7630.138256	9.195725	-0.150757	4.706432
785.746687	7638.111974	9.200730	-0.150913	4.708832
786.447942	7646.127640	9.205735	-0.151049	4.711243
787.073110	7654.145025	9.210739	-0.151170	4.713654
787.470425	7662.216863	9.215744	-0.151250	4.716080
788.416610	7670.164537	9.220749	-0.151431	4.718467
789.056155	7678.251251	9.225754	-0.151555	4.720895
789.547309	7686.233979	9.230759	-0.151652	4.723290
790.241702	7694.309122	9.235763	-0.151786	4.725712
790.618729	7702.264009	9.240768	-0.151861	4.728096
791.382588	7710.342257	9.245773	-0.152009	4.730516
792.129929	7718.319524	9.250778	-0.152153	4.732904
793.117362	7726.308639	9.255783	-0.152342	4.735294
793.949796	7734.345527	9.260787	-0.152502	4.737697
794.607009	7742.369417	9.265792	-0.152630	4.740095
794.862931	7750.448896	9.270797	-0.152683	4.742510
795.531818	7758.415676	9.275802	-0.152812	4.744888
796.228199	7766.401650	9.280807	-0.152947	4.747271
797.272162	7774.332904	9.285811	-0.153146	4.749636
797.474015	7782.470678	9.290816	-0.153189	4.752063
798.560657	7790.423647	9.295821	-0.153397	4.754431
799.206273	7798.497520	9.300826	-0.153522	4.756835
800.162662	7806.359203	9.305831	-0.153705	4.759174
801.057008	7814.551633	9.310835	-0.153877	4.761610
801.522326	7822.416061	9.315840	-0.153969	4.763949
802.076048	7830.561743	9.320845	-0.154077	4.766370
802.719002	7838.542724	9.325850	-0.154202	4.768740
803.889320	7846.540885	9.330855	-0.154425	4.771112
804.977414	7854.498273	9.335859	-0.154633	4.773471
806.071080	7862.525331	9.340864	-0.154841	4.775849
806.562451	7870.610976	9.345869	-0.154938	4.778246
807.384574	7878.629486	9.350874	-0.155096	4.780620
807.807543	7886.617372	9.355879	-0.155180	4.782986
808.773645	7894.637968	9.360883	-0.155365	4.785358
809.350065	7902.705991	9.365888	-0.155478	4.787744
810.185259	7910.702796	9.370893	-0.155638	4.790107
811.375967	7918.729066	9.375898	-0.155865	4.792475
812.158930	7926.708394	9.380903	-0.156016	4.794830
813.511917	7934.687716	9.385907	-0.156273	4.797182
814.146404	7942.692425	9.390912	-0.156396	4.799543
815.043087	7950.741294	9.395917	-0.156568	4.801914
816.159831	7958.701556	9.400922	-0.156781	4.804257
817.265922	7966.786727	9.405927	-0.156993	4.806636
817.941333	7974.820780	9.410931	-0.157123	4.809000
818.902135	7982.813797	9.415936	-0.157308	4.811350
819.588425	7990.164858	9.420941	-0.157440	4.813511
820.280221	7994.819878	9.425946	-0.157572	4.814877

820.949315	7997.338429	9.430951	-0.157698	4.815615
822.166104	7998.601227	9.435955	-0.157925	4.815981
822.723213	7999.027516	9.440960	-0.158029	4.816103
823.568101	8000.152797	9.445965	-0.158187	4.816430
824.466667	8000.133630	9.450970	-0.158354	4.816420
824.874289	8000.125480	9.455975	-0.158430	4.816416
825.652433	8000.155290	9.460979	-0.158575	4.816421
826.394671	8000.144170	9.465984	-0.158713	4.816414
826.818240	8000.160706	9.470989	-0.158792	4.816417
827.151330	8000.189551	9.475994	-0.158854	4.816424
828.116991	8000.117367	9.480999	-0.159033	4.816398
828.390100	8000.232281	9.486003	-0.159084	4.816430
828.452565	8000.215256	9.491008	-0.159096	4.816425
829.435169	8000.197505	9.496013	-0.159279	4.816415
829.665362	8000.253323	9.501018	-0.159321	4.816430
830.111789	8000.221409	9.506023	-0.159405	4.816419
830.717392	8000.220794	9.511027	-0.159517	4.816415
831.277611	8000.207751	9.516032	-0.159621	4.816409
831.229957	8000.245177	9.521037	-0.159612	4.816420
831.934354	8000.206915	9.526042	-0.159744	4.816405
831.548316	8000.261043	9.531047	-0.159672	4.816423
832.011032	8000.305849	9.536051	-0.159758	4.816434
832.347809	8000.224348	9.541056	-0.159820	4.816409
832.798811	8000.292322	9.546061	-0.159904	4.816426
833.482779	8000.237801	9.551066	-0.160031	4.816407
833.438740	8000.275289	9.556071	-0.160023	4.816418
834.078982	8000.258272	9.561075	-0.160142	4.816410
834.592809	8000.221112	9.566080	-0.160238	4.816397
834.725078	8000.230727	9.571085	-0.160262	4.816399
834.571233	8000.278078	9.576090	-0.160234	4.816414
834.799710	8000.270173	9.581095	-0.160276	4.816410
835.390460	8000.276763	9.586099	-0.160386	4.816409
835.694421	8000.244625	9.591104	-0.160443	4.816398
835.666093	8000.314230	9.596109	-0.160437	4.816419
836.008856	8000.318839	9.601114	-0.160501	4.816419
836.026652	8000.309569	9.606119	-0.160504	4.816416
836.629336	8000.334414	9.611123	-0.160616	4.816420
836.415144	8000.332981	9.616128	-0.160576	4.816421
836.804392	8000.379775	9.621133	-0.160649	4.816433
837.097362	8000.344272	9.626138	-0.160703	4.816421
837.024674	8000.363235	9.631143	-0.160690	4.816427
837.508428	8000.355319	9.636147	-0.160780	4.816422
837.587981	8000.351320	9.641152	-0.160794	4.816420
837.876195	8000.357153	9.646157	-0.160848	4.816421
837.990017	8000.367528	9.651162	-0.160869	4.816423
838.307364	8000.313316	9.656167	-0.160928	4.816406
838.859181	8000.320337	9.661171	-0.161031	4.816405
839.238939	8000.234241	9.666176	-0.161101	4.816378
839.031842	8000.346548	9.671181	-0.161063	4.816412
839.574156	8000.314122	9.676186	-0.161163	4.816400
839.582392	8000.236729	9.681191	-0.161165	4.816377
839.999787	8000.265948	9.686195	-0.161243	4.816384
839.647512	8000.284519	9.691200	-0.161177	4.816391
839.590247	8000.343030	9.696205	-0.161166	4.816408
839.983926	8000.351679	9.701210	-0.161239	4.816409
840.193952	8000.286130	9.706215	-0.161278	4.816389
840.501362	8000.346446	9.711219	-0.161336	4.816405
840.687107	8000.286866	9.716224	-0.161370	4.816386
841.049999	8000.229164	9.721229	-0.161437	4.816368
840.531601	8000.344801	9.726234	-0.161341	4.816404
840.894558	8000.343385	9.731239	-0.161408	4.816402
841.100635	8000.388216	9.736243	-0.161447	4.816414
840.881169	8000.366510	9.741248	-0.161406	4.816409
841.507657	8000.282388	9.746253	-0.161522	4.816381
841.275627	8000.392160	9.751258	-0.161479	4.816414
841.590210	8000.409059	9.756263	-0.161538	4.816418
841.566985	8000.412913	9.761267	-0.161533	4.816419
841.899208	8000.345145	9.766272	-0.161595	4.816398
842.199075	8000.329940	9.771277	-0.161651	4.816392
841.952888	8000.427795	9.776282	-0.161605	4.816422
842.207180	8000.409710	9.781287	-0.161652	4.816415
842.591999	8000.344940	9.786291	-0.161723	4.816394
842.425991	8000.364476	9.791296	-0.161692	4.816401
842.353853	8000.390883	9.796301	-0.161679	4.816409
842.949617	8000.372099	9.801306	-0.161790	4.816400
842.702530	8000.397722	9.806311	-0.161744	4.816409
842.814148	8000.438864	9.811315	-0.161764	4.816421
842.689582	8000.399615	9.816320	-0.161741	4.816410
843.336191	8000.449649	9.821325	-0.161862	4.816421
843.551155	8000.440469	9.826330	-0.161901	4.816418
843.768788	8000.342122	9.831335	-0.161942	4.816388
844.040372	8000.383801	9.836339	-0.161992	4.816399
843.699972	8000.422741	9.841344	-0.161929	4.816412
843.565631	8000.391824	9.846349	-0.161904	4.816403
844.167080	8000.410312	9.851354	-0.162016	4.816406
844.005955	8000.397004	9.856359	-0.161986	4.816403
843.653385	8000.439990	9.861363	-0.161920	4.816417
844.292031	8000.369883	9.866368	-0.162039	4.816393
844.092866	8000.416481	9.871373	-0.162001	4.816408
844.270212	8000.436415	9.876378	-0.162034	4.816413
844.395163	8000.410871	9.881383	-0.162058	4.816405
844.810921	8000.383790	9.886387	-0.162135	4.816395
844.539504	8000.384579	9.891392	-0.162084	4.816396
844.263601	8000.439459	9.896397	-0.162033	4.816414
844.817629	8000.413616	9.901402	-0.162136	4.816404
845.010550	8000.399824	9.906407	-0.162172	4.816399
845.180668	8000.403707	9.911411	-0.162203	4.816399
845.146594	8000.408443	9.916416	-0.162197	4.816400
845.409670	8000.395818	9.921421	-0.162246	4.816395
845.528551	8000.382918	9.926426	-0.162268	4.816391
845.571562	8000.340080	9.931431	-0.162276	4.816378
846.294751	8000.322365	9.936435	-0.162410	4.816370
846.275527	8000.350714	9.941440	-0.162407	4.816378
846.024767	8000.332726	9.946445	-0.162360	4.816374
846.437775	8000.327907	9.951450	-0.162437	4.816370
846.307080	8000.348029	9.956455	-0.162412	4.816377
846.373213	8000.390544	9.961459	-0.162424	4.816389
846.424671	8000.359529	9.966464	-0.162434	4.816380
846.949888	8000.256739	9.971469	-0.162532	4.816347
847.102176	8000.310248	9.976474	-0.162560	4.816362
846.834407	8000.301535	9.981479	-0.162510	4.816361
847.118086	8000.345547	9.986483	-0.162563	4.816372
846.799841	8000.386976	9.991488	-0.162503	4.816386
846.650508	8000.357930	9.996493	-0.162475	4.816378
847.110614	8000.354958	10.001498	-0.162561	4.816375
847.064941	8000.305332	10.006503	-0.162552	4.816361
847.046983	8000.361318	10.011507	-0.162549	4.816377
847.471337	8000.348194	10.016512	-0.162628	4.816371
847.117799	8000.428334	10.021517	-0.162562	4.816397
847.092647	8000.458709	10.026522	-0.162557	4.816406
846.489875	8000.489029	10.031527	-0.162445	4.816418
846.797527	8000.510074	10.036531	-0.162502	4.816422
847.272916	8000.452127	10.041536	-0.162591	4.816403
847.743450	8000.388790	10.046541	-0.162678	4.816382
847.690059	8000.448436	10.051546	-0.162668	4.816400
847.857740	8000.370496	10.056551	-0.162699	4.816376
848.228960	8000.373483	10.061555	-0.162768	4.816375
848.236995	8000.353428	10.066560	-0.162770	4.816369
848.251411	8000.351536	10.071565	-0.162772	4.816369
848.191639	8000.407890	10.076570	-0.162761	4.816385
847.877731	8000.422835	10.081575	-0.162703	4.816391
848.185465	8000.420517	10.086579	-0.162760	4.816389
848.341710	8000.391246	10.091584	-0.162789	4.816380
848.387247	8000.375002	10.096589	-0.162797	4.816375
848.757417	8000.408776	10.101594	-0.162866	4.816383
848.739940	8000.402104	10.106599	-0.162863	4.816381
848.409619	8000.480506	10.111603	-0.162801	4.816406
848.434023	8000.469221	10.116608	-0.162806	4.816402
848.744372	8000.423398	10.121613	-0.162863	4.816387
849.216372	8000.300605	10.126618	-0.162951	4.816349
848.973589	8000.309299	10.131623	-0.162906	4.816353
849.159565	8000.378244	10.136627	-0.162940	4.816372
849.366602	8000.343447	10.141632	-0.162979	4.816361
848.907918	8000.449451	10.146637	-0.162893	4.816394
848.693109	8000.489414	10.151642	-0.162853	4.816407
849.070778	8000.341682	10.156647	-0.162923	4.816362
849.454262	8000.373555	10.161651	-0.162995	4.816369
849.323444	8000.413855	10.166656	-0.162970	4.816382
849.275542	8000.417298	10.171661	-0.162961	4.816383
849.285738	8000.453575	10.176666	-0.162963	4.816394
848.785998	8000.507909	10.181671	-0.162870	4.816412
849.239651	8000.492092	10.186675	-0.162954	4.816405
849.750881	8000.448556	10.191680	-0.163049	4.816390
849.736790	8000.402638	10.196685	-0.163047	4.816376
849.687424	8000.510152	10.201690	-0.163037	4.816408
849.193369	8000.422247	10.206695	-0.162945	4.816385
849.013457	8000.581757	10.211699	-0.162912	4.816433
849.416677	8000.499244	10.216704	-0.162987	4.816406
849.114469	8000.419847	10.221709	-0.162930	4.816384
849.404482	8000.540450	10.226714	-0.162984	4.816419
849.350650	8000.471565	10.231719	-0.162974	4.816399
849.508674	8000.502870	10.236723	-0.163004	4.816407
849.397491	8000.487200	10.241728	-0.162983	4.816403
849.939083	8000.466477	10.246733	-0.163084	4.816394
849.394839	8000.526442	10.251738	-0.162982	4.816414
849.649341	8000.493498	10.256743	-0.163029	4.816404
850.440454	8000.470561	10.261747	-0.163177	4.816393
850.127216	8000.518443	10.266752	-0.163118	4.816409
850.020529	8000.520905	10.271757	-0.163098	4.816410
850.567315	8000.468404	10.276762	-0.163200	4.816392
850.364383	8000.438458	10.281767	-0.163162	4.816384
850.303936	8000.462935	10.286771	-0.163151	4.816391
850.823239	8000.448216	10.291776	-0.163247	4.816384
850.769387	8000.460057	10.296781	-0.163237	4.816388
850.815397	8000.488434	10.301786	-0.163246	4.816396
851.161462	8000.402844	10.306791	-0.163310	4.816370
851.310677	8000.465872	10.311795	-0.163338	4.816387
851.597868	8000.419666	10.316800	-0.163391	4.816372
851.323552	8000.455449	10.321805	-0.163340	4.816384
851.883039	8000.396788	10.326810	-0.163444	4.816364
852.017098	8000.314036	10.331815	-0.163469	4.816339
852.041912	8000.365430	10.336819	-0.163473	4.816354
852.006697	8000.411574	10.341824	-0.163467	4.816368
851.553576	8000.454997	10.346829	-0.163382	4.816383
851.605914	8000.471795	10.351834	-0.163392	4.816388
851.797355	8000.386814	10.356839	-0.163428	4.816362
852.111754	8000.366555	10.361843	-0.163486	4.816354
852.070398	8000.415784	10.366848	-0.163478	4.816369
851.802638	8000.419808	10.371853	-0.163428	4.816371
851.630037	8000.496590	10.376858	-0.163396	4.816395
851.763149	8000.459499	10.381863	-0.163421	4.816383
851.558815	8000.470955	10.386867	-0.163383	4.816388
851.280499	8000.406820	10.391872	-0.163331	4.816370
851.837378	8000.479834	10.396877	-0.163434	4.816389
851.793941	8000.509907	10.401882	-0.163426	4.816398
851.794143	8000.482284	10.406887	-0.163426	4.816390
851.928477	8000.530194	10.411891	-0.163451	4.816403
852.277639	8000.488209	10.416896	-0.163516	4.816389
852.395741	8000.443432	10.421901	-0.163538	4.816375
852.421636	8000.500157	10.426906	-0.163543	4.816392
852.120545	8000.476005	10.431911	-0.163486	4.816386
852.176915	8000.538549	10.436915	-0.163497	4.816404
852.105171	8000.437491	10.441920	-0.163483	4.816375
852.612058	8000.482057	10.446925	-0.163578	4.816386
852.513869	8000.496345	10.451930	-0.163559	4.816390
852.304830	8000.489662	10.456935	-0.163520	4.816389
852.873565	8000.408850	10.461939	-0.163626	4.816363
852.728140	8000.445720	10.466944	-0.163599	4.816375
852.486311	8000.480982	10.471949	-0.163554	4.816386
852.600508	8000.504125	10.476954	-0.163575	4.816392
853.325442	8000.406799	10.481959	-0.163710	4.816360
853.122789	8000.446963	10.486963	-0.163672	4.816373
852.955049	8000.512142	10.491968	-0.163641	4.816393
853.112761	8000.497770	10.496973	-0.163670	4.816388
853.286361	8000.539964	10.501978	-0.163702	4.816399
853.319131	8000.443834	10.506983	-0.163708	4.816371
853.256518	8000.458716	10.511987	-0.163697	4.816376
853.035162	8000.558056	10.516992	-0.163655	4.816406
852.932950	8000.569089	10.521997	-0.163636	4.816410
853.314917	8000.525529	10.527002	-0.163707	4.816395
853.531690	8000.433533	10.532007	-0.163747	4.816367
853.321014	8000.520304	10.537011	-0.163708	4.816394
853.238715	8000.515735	10.542016	-0.163693	4.816393
853.099964	8000.442238	10.547021	-0.163667	4.816372
853.620498	8000.555024	10.552026	-0.163764	4.816402
853.185504	8000.569000	10.557031	-0.163683	4.816409
853.545931	8000.571822	10.562035	-0.163750	4.816408
853.418357	8000.553750	10.567040	-0.163726	4.816403
853.458221	8000.406749	10.572045	-0.163733	4.816360
853.444992	8000.563740	10.577050	-0.163731	4.816406
853.490443	8000.512438	10.582055	-0.163739	4.816390
853.656782	8000.533266	10.587059	-0.163770	4.816396
853.524945	8000.535306	10.592064	-0.163745	4.816397
853.275955	8000.461031	10.597069	-0.163699	4.816376
853.814768	8000.515696	10.602074	-0.163799	4.816390
853.431480	8000.532660	10.607079	-0.163728	4.816397
853.377438	8000.583803	10.612083	-0.163717	4.816412
853.536001	8000.461091	10.617088	-0.163747	4.816375
853.660667	8000.576830	10.622093	-0.163770	4.816409
853.900573	8000.537273	10.627098	-0.163814	4.816396
853.513063	8000.547793	10.632103	-0.163742	4.816401
853.773023	8000.452268	10.637107	-0.163791	4.816371
853.964378	8000.541501	10.642112	-0.163826	4.816397
854.285265	8000.478863	10.647117	-0.163886	4.816377
854.198255	8000.517771	10.652122	-0.163869	4.816389
853.950984	8000.506198	10.657127	-0.163823	4.816386
854.093518	8000.546813	10.662131	-0.163850	4.816398
853.701800	8000.487150	10.667136	-0.163777	4.816382
853.840362	8000.435278	10.672141	-0.163802	4.816366
854.022033	8000.566842	10.677146	-0.163836	4.816404
854.018379	8000.517907	10.682151	-0.163835	4.816389
854.491584	8000.544922	10.687155	-0.163923	4.816395
854.433468	8000.532258	10.692160	-0.163913	4.816392
854.514132	8000.525099	10.697165	-0.163928	4.816389
854.545815	8000.470379	10.702170	-0.163933	4.816373
854.274432	8000.521080	10.707175	-0.163883	4.816389
854.289007	8000.578681	10.712179	-0.163885	4.816406
854.527955	8000.408443	10.717184	-0.163930	4.816355
854.209181	8000.511469	10.722189	-0.163870	4.816387
854.457420	8000.605904	10.727194	-0.163916	4.816413
854.775111	8000.543213	10.732199	-0.163975	4.816393
855.071870	8000.413245	10.737203	-0.164031	4.816354
855.086587	8000.489971	10.742208	-0.164033	4.816376
854.886920	8000.530184	10.747213	-0.163996	4.816389
855.003066	8000.535303	10.752218	-0.164018	4.816390
854.758032	8000.498270	10.757223	-0.163972	4.816380
854.660897	8000.465832	10.762227	-0.163954	4.816371
855.134899	8000.474803	10.767232	-0.164042	4.816371
854.896550	8000.488874	10.772237	-0.163997	4.816377
855.292657	8000.462550	10.777242	-0.164071	4.816367
856.032188	8000.431340	10.782247	-0.164209	4.816354
855.624251	8000.544562	10.787251	-0.164133	4.816389
855.853101	8000.504822	10.792256	-0.164175	4.816377
855.833409	8000.487487	10.797261	-0.164171	4.816372
855.461415	8000.481264	10.802266	-0.164102	4.816372
855.762327	8000.496907	10.807271	-0.164158	4.816375
855.665482	8000.546274	10.812275	-0.164140	4.816390
855.828610	8000.556428	10.817280	-0.164170	4.816392
855.887105	8000.416105	10.822285	-0.164181	4.816350
855.943535	8000.491404	10.827290	-0.164191	4.816372
855.873460	8000.527408	10.832295	-0.164178	4.816383
856.149457	8000.460834	10.837299	-0.164230	4.816362
856.276107	8000.458693	10.842304	-0.164253	4.816361
855.918103	8000.467576	10.847309	-0.164186	4.816365
856.358985	8000.507868	10.852314	-0.164268	4.816375
855.692097	8000.503091	10.857319	-0.164144	4.816377
855.553660	8000.549639	10.862323	-0.164118	4.816391
855.667015	8000.468661	10.867328	-0.164139	4.816367
855.735833	8000.582413	10.872333	-0.164152	4.816400
855.623817	8000.445615	10.877338	-0.164131	4.816360
855.284847	8000.510059	10.882343	-0.164068	4.816381
855.670255	8000.501617	10.887347	-0.164139	4.816377
856.372636	8000.530343	10.892352	-0.164270	4.816382
856.304671	8000.502640	10.897357	-0.164257	4.816374
856.151733	8000.440584	10.902362	-0.164229	4.816356
855.987382	8000.465452	10.907367	-0.164198	4.816365
855.879405	8000.551816	10.912371	-0.164178	4.816390
855.959952	8000.488350	10.917376	-0.164193	4.816371
856.023118	8000.555264	10.922381	-0.164205	4.816391
856.003403	8000.559176	10.927386	-0.164201	4.816392
856.207977	8000.524341	10.932391	-0.164239	4.816381
856.592496	8000.425585	10.937395	-0.164310	4.816350
856.614280	8000.549176	10.942400	-0.164314	4.816386
856.558767	8000.481311	10.947405	-0.164304	4.816366
856.566716	8000.470812	10.952410	-0.164305	4.816363
857.070398	8000.428228	10.957415	-0.164399	4.816348
856.753338	8000.580153	10.962419	-0.164340	4.816394
857.198869	8000.504727	10.967424	-0.164423	4.816370
857.264363	8000.415511	10.972429	-0.164435	4.816344
856.865208	8000.474699	10.977434	-0.164360	4.816363
857.097577	8000.432893	10.982439	-0.164403	4.816350
856.654054	8000.578454	10.987443	-0.164321	4.816394
856.394906	8000.487001	10.992448	-0.164272	4.816369
856.966452	8000.456175	10.997453	-0.164379	4.816357
857.081694	8000.539897	11.002458	-0.164400	4.816381
857.023717	8000.532545	11.007463	-0.164389	4.816379
856.825766	8000.456987	11.012467	-0.164352	4.816358
856.784112	8000.591205	11.017472	-0.164345	4.816398
856.941296	8000.533269	11.022477	-0.164374	4.816380
856.574587	8000.424081	11.027482	-0.164305	4.816350
856.563599	8000.524815	11.032487	-0.164303	4.816379
857.102262	8000.547622	11.037491	-0.164403	4.816383
857.474881	8000.554906	11.042496	-0.164473	4.816384
857.149137	8000.433652	11.047501	-0.164412	4.816350
856.675492	8000.457599	11.052506	-0.164324	4.816359
857.132085	8000.515155	11.057511	-0.164409	4.816374
856.989274	8000.613687	11.062515	-0.164382	4.816403
857.129248	8000.472596	11.067520	-0.164408	4.816361
857.380189	8000.528841	11.072525	-0.164455	4.816376
857.224437	8000.492232	11.077530	-0.164425	4.816366
857.077260	8000.475953	11.082535	-0.164398	4.816362
857.509274	8000.564972	11.087539	-0.164478	4.816386
857.381957	8000.547962	11.092544	-0.164455	4.816382
857.102944	8000.563475	11.097549	-0.164403	4.816388
856.866662	8000.480901	11.102554	-0.164358	4.816365
857.114916	8000.541349	11.107559	-0.164405	4.816381
856.998552	8000.478840	11.112563	-0.164383	4.816364
856.848546	8000.327592	11.117568	-0.164355	4.816320
856.880693	8000.634087	11.122573	-0.164361	4.816410
857.236945	8000.497675	11.127578	-0.164427	4.816368
857.245792	8000.514813	11.132583	-0.164428	4.816373
857.194257	8000.373709	11.137587	-0.164419	4.816332
857.364799	8000.406298	11.142592	-0.164450	4.816340
857.552205	8000.485915	11.147597	-0.164485	4.816363
857.318862	8000.402327	11.152602	-0.164442	4.816340
857.483107	8000.512367	11.157607	-0.164472	4.816371
857.465078	8000.423879	11.162611	-0.164469	4.816345
856.958964	8000.398413	11.167616	-0.164374	4.816340
857.157652	8000.428285	11.172621	-0.164411	4.816348
857.802833	8000.527243	11.177626	-0.164531	4.816374
857.710471	8000.508692	11.182631	-0.164514	4.816369
857.570284	8000.501028	11.187635	-0.164488	4.816367
858.054353	8000.493178	11.192640	-0.164578	4.816363
857.766193	8000.546784	11.197645	-0.164524	4.816380
857.554568	8000.380691	11.202650	-0.164485	4.816332
857.740923	8000.461354	11.207655	-0.164519	4.816355
857.710448	8000.396030	11.212659	-0.164514	4.816336
858.003683	8000.509290	11.217664	-0.164568	4.816368
858.004617	8000.451928	11.222669	-0.164568	4.816351
858.430481	8000.486664	11.227674	-0.164647	4.816359
858.017194	8000.511617	11.232679	-0.164570	4.816368
858.174868	8000.478124	11.237683	-0.164600	4.816358
858.661619	8000.587188	11.242688	-0.164690	4.816387
857.776492	8000.524567	11.247693	-0.164525	4.816373
858.018214	8000.400050	11.252698	-0.164570	4.816335
858.615613	8000.542835	11.257703	-0.164681	4.816375
858.513418	8000.474185	11.262707	-0.164662	4.816355
858.196999	8000.488009	11.267712	-0.164603	4.816360
857.930049	8000.410231	11.272717	-0.164553	4.816339
858.368518	8000.496173	11.277722	-0.164635	4.816362
858.381783	8000.568632	11.282727	-0.164637	4.816383
858.435637	8000.421849	11.287731	-0.164647	4.816340
858.551398	8000.626700	11.292736	-0.164669	4.816399
858.838844	8000.417952	11.297741	-0.164722	4.816337
858.452821	8000.512418	11.302746	-0.164650	4.816366
858.544727	8000.482075	11.307751	-0.164667	4.816357
858.865192	8000.614919	11.312755	-0.164727	4.816394
858.554300	8000.441847	11.317760	-0.164669	4.816345
858.606454	8000.436337	11.322765	-0.164678	4.816343
858.489159	8000.400370	11.327770	-0.164657	4.816333
858.711075	8000.485880	11.332775	-0.164698	4.816357
858.614646	8000.386516	11.337779	-0.164680	4.816329
858.957988	8000.510181	11.342784	-0.164744	4.816363
859.102915	8000.600780	11.347789	-0.164771	4.816389
859.091164	8000.410399	11.352794	-0.164768	4.816333
859.002191	8000.501335	11.357799	-0.164752	4.816360
859.371691	8000.576568	11.362803	-0.164820	4.816381
859.383650	8000.498139	11.367808	-0.164822	4.816358
859.362542	8000.451030	11.372813	-0.164818	4.816344
859.460551	8000.578031	11.377818	-0.164837	4.816381
859.985193	8000.490120	11.382823	-0.164934	4.816352
859.926769	8000.400951	11.387827	-0.164923	4.816326
859.508225	8000.490622	11.392832	-0.164845	4.816355
859.868593	8000.525331	11.397837	-0.164912	4.816363
859.661168	8000.551600	11.402842	-0.164874	4.816372
859.920193	8000.498555	11.407847	-0.164922	4.816355
859.697965	8000.442768	11.412851	-0.164880	4.816340
859.293648	8000.599611	11.417856	-0.164805	4.816388
858.728963	8000.526409	11.422861	-0.164700	4.816369
858.948624	8000.387711	11.427866	-0.164740	4.816327
859.006268	8000.520408	11.432871	-0.164751	4.816366
859.396336	8000.393059	11.437875	-0.164823	4.816327
859.784846	8000.590793	11.442880	-0.164896	4.816383
859.693647	8000.539323	11.447885	-0.164879	4.816368
859.559451	8000.466948	11.452890	-0.164854	4.816348
859.123780	8000.464963	11.457895	-0.164772	4.816349
859.849435	8000.476034	11.462899	-0.164907	4.816349
859.784678	8000.504692	11.467904	-0.164895	4.816358
859.320437	8000.476729	11.472909	-0.164809	4.816352
859.695999	8000.511691	11.477914	-0.164879	4.816360
859.463873	8000.499300	11.482919	-0.164835	4.816358
859.477170	8000.502702	11.487923	-0.164838	4.816359
859.785626	8000.488731	11.492928	-0.164895	4.816353
859.652541	8000.562993	11.497933	-0.164870	4.816375
859.509701	8000.535096	11.502938	-0.164844	4.816368
859.057403	8000.418089	11.507943	-0.164759	4.816336
859.290413	8000.417730	11.512947	-0.164802	4.816335
859.375086	8000.462698	11.517952	-0.164818	4.816347
859.450785	8000.496893	11.522957	-0.164832	4.816357
859.563807	8000.406343	11.527962	-0.164853	4.816330
859.824992	8000.529700	11.532967	-0.164902	4.816365
859.320728	8000.424572	11.537971	-0.164808	4.816336
859.626470	8000.542299	11.542976	-0.164865	4.816370
859.791375	8000.494053	11.547981	-0.164895	4.816355
859.592276	8000.491776	11.552986	-0.164858	4.816355
859.497648	8000.431750	11.557991	-0.164840	4.816338
859.709852	8000.507539	11.562995	-0.164880	4.816359
859.925473	8000.445267	11.568000	-0.164920	4.816340
859.752016	8000.422171	11.573005	-0.164887	4.816334
860.115085	8000.598232	11.578010	-0.164955	4.816384
859.736091	8000.511134	11.583015	-0.164884	4.816360
859.689099	8000.524152	11.588019	-0.164875	4.816364
858.998996	8000.146061	11.593024	-0.164747	4.816256
859.115703	8000.305243	11.598029	-0.164768	4.816302
859.336908	8000.114512	11.603034	-0.164809	4.816245
859.165407	8000.191317	11.608039	-0.164777	4.816269
859.185332	8000.172519	11.613043	-0.164781	4.816263
859.540378	8000.350562	11.618048	-0.164847	4.816314
859.651356	8000.409783	11.623053	-0.164868	4.816330
859.686289	8000.294554	11.628058	-0.164874	4.816296
860.235935	8000.607605	11.633063	-0.164977	4.816386
859.755718	8000.263826	11.638067	-0.164887	4.816287
859.381647	8000.237375	11.643072	-0.164817	4.816281
859.233199	8000.149891	11.648077	-0.164789	4.816256
859.356346	8000.265622	11.653082	-0.164812	4.816290
859.584741	8000.266247	11.658087	-0.164855	4.816289
860.010256	8000.430599	11.663091	-0.164934	4.816335
860.017862	8000.323411	11.668096	-0.164935	4.816303
859.112810	8000.220083	11.673101	-0.164766	4.816277
859.566298	8000.176663	11.678106	-0.164851	4.816262
859.647139	8000.403243	11.683111	-0.164866	4.816329
859.583563	8000.228995	11.688115	-0.164854	4.816278
860.064234	8000.248714	11.693120	-0.164943	4.816281
860.477450	8000.528673	11.698125	-0.165020	4.816361
860.621952	8000.516209	11.703130	-0.165047	4.816357
860.160355	8000.406479	11.708135	-0.164961	4.816327
860.144083	8000.414698	11.713139	-0.164958	4.816330
860.961361	8000.476181	11.718144	-0.165110	4.816344
860.760328	8000.517432	11.723149	-0.165073	4.816357
860.353153	8000.412861	11.728154	-0.164997	4.816328
860.309038	8000.561922	11.733159	-0.164988	4.816372
860.247548	8000.450389	11.738163	-0.164977	4.816340
859.703813	8000.335038	11.743168	-0.164875	4.816308
860.481833	8000.400109	11.748173	-0.165020	4.816324
860.844355	8000.537916	11.753178	-0.165088	4.816362
860.135818	8000.351804	11.758183	-0.164956	4.816311
860.563553	8000.540636	11.763187	-0.165035	4.816365
860.977232	8000.433869	11.768192	-0.165112	4.816331
860.904066	8000.499572	11.773197	-0.165098	4.816351
860.883377	8000.467344	11.778202	-0.165094	4.816341
861.134534	8000.476853	11.783207	-0.165141	4.816343
861.050697	8000.612502	11.788211	-0.165126	4.816383
860.696774	8000.428072	11.793216	-0.165059	4.816331
860.721945	8000.542170	11.798221	-0.165064	4.816364
860.353193	8000.418056	11.803226	-0.164995	4.816330
859.873327	8000.378144	11.808231	-0.164906	4.816320
860.241146	8000.409790	11.813235	-0.164974	4.816328
860.248720	8000.192107	11.818240	-0.164975	4.816264
860.300096	8000.393761	11.823245	-0.164985	4.816323
860.704396	8000.436644	11.828250	-0.165060	4.816333
860.605441	8000.460479	11.833255	-0.165042	4.816341
861.030839	8000.433593	11.838259	-0.165121	4.816331
861.132987	8000.530919	11.843264	-0.165140	4.816359
860.899636	8000.494067	11.848269	-0.165096	4.816349
860.871567	8000.400092	11.853274	-0.165091	4.816322
860.861506	8000.505100	11.858279	-0.165089	4.816353
860.896173	8000.525860	11.863283	-0.165095	4.816359
861.194198	8000.497905	11.868288	-0.165151	4.816349
861.182068	8000.580568	11.873293	-0.165148	4.816373
861.020554	8000.423796	11.878298	-0.165118	4.816328
861.109798	8000.554905	11.883303	-0.165135	4.816366
861.046272	8000.411461	11.888307	-0.165123	4.816324
861.036580	8000.411291	11.893312	-0.165121	4.816324
860.606019	8000.520947	11.898317	-0.165041	4.816359
861.334679	8000.497015	11.903322	-0.165176	4.816348
860.973076	8000.426141	11.908327	-0.165109	4.816329
860.625095	8000.325749	11.913331	-0.165044	4.816301
860.831022	8000.368499	11.918336	-0.165082	4.816313
860.729933	8000.402923	11.923341	-0.165063	4.816323
860.852912	8000.401786	11.928346	-0.165086	4.816322
860.879658	8000.499973	11.933351	-0.165091	4.816351
861.225837	8000.471762	11.938355	-0.165155	4.816341
861.163150	8000.387831	11.943360	-0.165144	4.816317
861.478824	8000.452608	11.948365	-0.165202	4.816334
861.455152	8000.569077	11.953370	-0.165198	4.816369
861.421689	8000.429323	11.958375	-0.165191	4.816328
860.865823	8000.276576	11.963379	-0.165088	4.816286
861.705965	8000.557317	11.968384	-0.165244	4.816364
861.395745	8000.476677	11.973389	-0.165186	4.816342
861.357967	8000.551473	11.978394	-0.165179	4.816364
861.461009	8000.468191	11.983399	-0.165198	4.816339
862.137530	8000.460388	11.988403	-0.165324	4.816333
862.093476	8000.517018	11.993408	-0.165316	4.816350
862.008611	8000.392338	11.998413	-0.165300	4.816314
862.023158	8000.577450	12.003418	-0.165303	4.816368
862.063557	8000.532431	12.008423	-0.165310	4.816355
862.343793	8000.422366	12.013427	-0.165362	4.816321
862.782269	8000.491329	12.018432	-0.165444	4.816339
862.436854	8000.511035	12.023437	-0.165379	4.816347
862.475978	8000.545683	12.028442	-0.165387	4.816357
862.377552	8000.463275	12.033447	-0.165368	4.816333
862.261144	8000.443255	12.038451	-0.165346	4.816328
861.468559	8000.333287	12.043456	-0.165199	4.816299
861.258938	8000.417956	12.048461	-0.165160	4.816325
861.988240	8000.509848	12.053466	-0.165295	4.816349
861.776430	8000.441480	12.058471	-0.165256	4.816330
861.666171	8000.386501	12.063475	-0.165235	4.816314
861.832089	8000.497646	12.068480	-0.165266	4.816346
862.271314	8000.547496	12.073485	-0.165348	4.816358
862.053019	8000.490706	12.078490	-0.165307	4.816343
861.483645	8000.409975	12.083495	-0.165201	4.816322
861.603485	8000.287663	12.088499	-0.165223	4.816285
861.455799	8000.416931	12.093504	-0.165195	4.816324
862.136817	8000.381577	12.098509	-0.165322	4.816310
862.145545	8000.537904	12.103514	-0.165324	4.816356
861.873307	8000.473836	12.108519	-0.165273	4.816339
861.978424	8000.471338	12.113523	-0.165292	4.816337
862.163015	8000.516923	12.118528	-0.165327	4.816350
862.045161	8000.595691	12.123533	-0.165305	4.816374
861.986777	8000.435330	12.128538	-0.165294	4.816327
862.088625	8000.528403	12.133543	-0.165313	4.816354
861.734053	8000.245146	12.138547	-0.165246	4.816272
861.842463	8000.394639	12.143552	-0.165267	4.816315
861.461629	8000.234195	12.148557	-0.165195	4.816270
861.733856	8000.271681	12.153562	-0.165246	4.816280
862.010631	8000.521744	12.158567	-0.165298	4.816352
862.158816	8000.385030	12.163571	-0.165325	4.816311
861.920225	8000.423527	12.168576	-0.165281	4.816324
862.006073	8000.477019	12.173581	-0.165297	4.816339
862.240043	8000.396992	12.178586	-0.165340	4.816314
861.813261	8000.280400	12.183591	-0.165260	4.816282
861.630817	8000.190215	12.188595	-0.165226	4.816256
861.880450	8000.320822	12.193600	-0.165273	4.816294
862.146724	8000.427273	12.198605	-0.165322	4.816324
862.197760	8000.262370	12.203610	-0.165332	4.816275
861.877301	8000.202809	12.208615	-0.165272	4.816259
861.826379	8000.245511	12.213619	-0.165262	4.816272
862.090250	8000.320045	12.218624	-0.165311	4.816292
862.250675	8000.428974	12.223629	-0.165341	4.816324
862.221623	8000.435917	12.228634	-0.165336	4.816326
862.017948	8000.318811	12.233639	-0.165298	4.816292
862.039869	8000.358482	12.238643	-0.165302	4.816304
862.112978	8000.399011	12.243648	-0.165315	4.816315
861.917691	8000.490295	12.248653	-0.165279	4.816343
861.936563	8000.427916	12.253658	-0.165282	4.816325
862.149701	8000.296540	12.258663	-0.165322	4.816285
861.812460	8000.346135	12.263667	-0.165259	4.816301
862.200482	8000.309062	12.268672	-0.165331	4.816289
862.298264	8000.456255	12.273677	-0.165349	4.816331
862.193213	8000.365237	12.278682	-0.165329	4.816305
862.071611	8000.347255	12.283687	-0.165307	4.816301
861.928188	8000.336346	12.288691	-0.165280	4.816298
862.529410	8000.434595	12.293696	-0.165392	4.816324
862.085625	8000.415466	12.298701	-0.165309	4.816320
862.133125	8000.302566	12.303706	-0.165318	4.816287
861.784411	8000.231908	12.308711	-0.165253	4.816268
862.045843	8000.165091	12.313715	-0.165301	4.816247
862.177476	8000.221473	12.318720	-0.165326	4.816263
862.333971	8000.195399	12.323725	-0.165355	4.816255
862.286071	8000.302963	12.328730	-0.165346	4.816286
861.935762	8000.179153	12.333735	-0.165280	4.816252
862.182757	8000.359655	12.338739	-0.165326	4.816304
862.250113	8000.172713	12.343744	-0.165339	4.816248
862.321734	8000.458655	12.348749	-0.165352	4.816332
862.480069	8000.370986	12.353754	-0.165382	4.816306
862.906578	8000.475874	12.358759	-0.165461	4.816334
862.575840	8000.434200	12.363763	-0.165399	4.816324
862.399916	8000.397244	12.368768	-0.165366	4.816314
862.622659	8000.485969	12.373773	-0.165408	4.816339
863.311983	8000.517699	12.378778	-0.165536	4.816345
862.634667	8000.378840	12.383783	-0.165410	4.816307
862.685782	8000.460440	12.388787	-0.165419	4.816331
863.172578	8000.421837	12.393792	-0.165510	4.816317
863.026754	8000.512888	12.398797	-0.165483	4.816345
862.788234	8000.381381	12.403802	-0.165438	4.816307
863.088188	8000.416149	12.408807	-0.165494	4.816316
862.654189	8000.370620	12.413811	-0.165413	4.816305
862.311607	8000.224624	12.418816	-0.165349	4.816263
862.621822	8000.381749	12.423821	-0.165407	4.816308
862.541864	8000.112652	12.428826	-0.165392	4.816229
862.310320	8000.203329	12.433831	-0.165348	4.816257
862.522406	8000.357748	12.438835	-0.165388	4.816301
862.662631	8000.234713	12.443840	-0.165414	4.816265
862.978067	8000.412116	12.448845	-0.165473	4.816315
863.077213	8000.348955	12.453850	-0.165491	4.816296
862.620972	8000.236116	12.458855	-0.165406	4.816265
863.026221	8000.382085	12.463859	-0.165481	4.816306
862.850473	8000.324945	12.468864	-0.165448	4.816290
862.689647	8000.480558	12.473869	-0.165419	4.816337
862.727321	8000.270803	12.478874	-0.165425	4.816275
862.818330	8000.451885	12.483879	-0.165442	4.816328
862.870322	8000.387934	12.488883	-0.165452	4.816309
862.572654	8000.164064	12.493888	-0.165396	4.816244
862.769904	8000.275735	12.498893	-0.165433	4.816276
863.104467	8000.452397	12.503898	-0.165495	4.816326
862.870944	8000.345412	12.508903	-0.165452	4.816296
863.155533	8000.428799	12.513907	-0.165505	4.816319
862.945299	8000.209578	12.518912	-0.165465	4.816256
863.140544	8000.534785	12.523917	-0.165502	4.816350
863.408493	8000.387325	12.528922	-0.165551	4.816306
862.933723	8000.298611	12.533927	-0.165463	4.816282
862.636764	8000.291504	12.538931	-0.165407	4.816281
862.653965	8000.152597	12.543936	-0.165410	4.816241
862.465938	8000.250378	12.548941	-0.165375	4.816270
862.549579	8000.156146	12.553946	-0.165391	4.816242
862.538517	8000.322765	12.558951	-0.165389	4.816291
862.641280	8000.169353	12.563955	-0.165408	4.816246
862.622676	8000.140346	12.568960	-0.165404	4.816237
862.471593	8000.191995	12.573965	-0.165376	4.816253
862.692570	8000.141500	12.578970	-0.165417	4.816237
862.400827	8000.081358	12.583975	-0.165363	4.816221
862.233867	8000.043493	12.588979	-0.165331	4.816211
862.457435	7999.940980	12.593984	-0.165373	4.816179
862.568290	8000.140450	12.598989	-0.165394	4.816237
862.859305	8000.229253	12.603994	-0.165448	4.816262
862.620176	8000.166803	12.608999	-0.165403	4.816245
862.534776	8000.195115	12.614003	-0.165387	4.816254
862.544396	7999.961521	12.619008	-0.165389	4.816185
862.441279	8000.156347	12.624013	-0.165369	4.816243
862.771261	8000.144864	12.629018	-0.165431	4.816238
862.828073	8000.215933	12.634023	-0.165441	4.816258
862.494433	8000.120026	12.639027	-0.165379	4.816232
862.798800	8000.196302	12.644032	-0.165436	4.816253
862.533016	8000.039907	12.649037	-0.165386	4.816208
862.600891	8000.153659	12.654042	-0.165399	4.816241
862.671656	8000.145274	12.659047	-0.165412	4.816238
862.674486	8000.010377	12.664051	-0.165412	4.816199
862.904496	8000.253283	12.669056	-0.165455	4.816269
862.953797	8000.344414	12.674061	-0.165464	4.816296
863.227295	8000.138610	12.679066	-0.165515	4.816234
863.057525	8000.289823	12.684071	-0.165483	4.816279
862.720991	8000.197053	12.689075	-0.165420	4.816253
862.675714	7999.944476	12.694080	-0.165412	4.816179
862.535949	8000.026064	12.699085	-0.165386	4.816204
862.717453	8000.085407	12.704090	-0.165419	4.816221
863.069954	8000.077489	12.709095	-0.165485	4.816217
863.148111	8000.112791	12.714099	-0.165499	4.816227
863.326247	8000.176329	12.719104	-0.165533	4.816244
863.198896	8000.274065	12.724109	-0.165509	4.816274
862.770764	8000.019323	12.729114	-0.165429	4.816201
863.151203	8000.217999	12.734119	-0.165500	4.816257
863.218059	8000.143673	12.739123	-0.165512	4.816235
862.926735	8000.068661	12.744128	-0.165458	4.816215
863.282844	8000.301995	12.749133	-0.165524	4.816281
863.082120	8000.105247	12.754138	-0.165486	4.816225
862.887862	8000.022299	12.759143	-0.165450	4.816201
862.822059	8000.155064	12.764147	-0.165438	4.816241
863.125718	7999.835017	12.769152	-0.165494	4.816145
863.390122	8000.146500	12.774157	-0.165544	4.816235
863.573387	8000.256876	12.779162	-0.165578	4.816267
863.366740	8000.105717	12.784167	-0.165539	4.816223
863.593412	8000.209382	12.789171	-0.165581	4.816253
863.633471	8000.381113	12.794176	-0.165589	4.816303
863.445876	8000.385399	12.799181	-0.165554	4.816305
863.535496	8000.244514	12.804186	-0.165570	4.816263
863.514850	8000.439666	12.809191	-0.165566	4.816321
863.347390	8000.290223	12.814195	-0.165535	4.816278
863.311245	8000.213108	12.819200	-0.165528	4.816255
863.294122	8000.150125	12.824205	-0.165525	4.816237
863.636403	8000.337543	12.829210	-0.165589	4.816290
863.814145	8000.214072	12.834215	-0.165621	4.816253
864.057313	8000.425334	12.839219	-0.165667	4.816314
863.350855	8000.154231	12.844224	-0.165535	4.816238
863.624694	8000.315002	12.849229	-0.165586	4.816284
863.466407	8000.059462	12.854234	-0.165556	4.816209
863.514800	8000.215392	12.859239	-0.165565	4.816255
863.444167	8000.066511	12.864243	-0.165552	4.816212
863.779356	8000.109306	12.869248	-0.165614	4.816222
863.484799	8000.224429	12.874253	-0.165559	4.816258
863.329519	8000.023130	12.879258	-0.165530	4.816199
863.546386	8000.143631	12.884263	-0.165571	4.816234
863.517169	8000.108070	12.889267	-0.165565	4.816223
863.767402	8000.127129	12.894272	-0.165612	4.816228
863.741037	8000.129867	12.899277	-0.165607	4.816229
863.801495	8000.102184	12.904282	-0.165618	4.816220
863.914032	8000.389883	12.909287	-0.165639	4.816304
864.158422	8000.371658	12.914291	-0.165684	4.816298
864.411172	8000.345072	12.919296	-0.165731	4.816289
864.457144	8000.504156	12.924301	-0.165740	4.816335
864.503921	8000.358299	12.929306	-0.165748	4.816292
864.715005	8000.424521	12.934311	-0.165788	4.816310
864.656356	8000.339587	12.939315	-0.165777	4.816286
864.162197	8000.416301	12.944320	-0.165684	4.816311
864.173670	8000.342106	12.949325	-0.165686	4.816289
864.342597	8000.297115	12.954330	-0.165718	4.816275
864.282918	8000.326921	12.959335	-0.165707	4.816284
864.093155	8000.397048	12.964339	-0.165671	4.816306
864.621665	8000.296456	12.969344	-0.165769	4.816273
864.326692	8000.410510	12.974349	-0.165715	4.816308
864.097106	8000.166519	12.979354	-0.165672	4.816238
864.164037	8000.220760	12.984359	-0.165684	4.816253
864.139798	8000.244784	12.989363	-0.165679	4.816261
864.401658	8000.235351	12.994368	-0.165728	4.816256
864.254813	8000.378452	12.999373	-0.165701	4.816299
864.122799	8000.146722	13.004378	-0.165676	4.816232
863.544199	8000.007394	13.009383	-0.165568	4.816194
863.653983	8000.168603	13.014387	-0.165588	4.816241
864.213270	8000.032398	13.019392	-0.165692	4.816198
864.076560	8000.169292	13.024397	-0.165667	4.816239
864.262765	8000.232968	13.029402	-0.165702	4.816256
864.347987	8000.211013	13.034407	-0.165717	4.816250
864.068163	8000.143626	13.039411	-0.165665	4.816231
864.267831	8000.327596	13.044416	-0.165702	4.816284
863.925296	8000.108279	13.049421	-0.165638	4.816222
863.955450	8000.116214	13.054426	-0.165644	4.816224
863.882142	8000.207418	13.059431	-0.165630	4.816251
864.036401	8000.251433	13.064435	-0.165659	4.816263
864.251566	8000.049961	13.069440	-0.165699	4.816203
864.460217	8000.407277	13.074445	-0.165738	4.816307
864.635245	8000.356013	13.079450	-0.165770	4.816291
865.145230	8000.398557	13.084455	-0.165865	4.816301
865.557183	8000.455399	13.089459	-0.165942	4.816315
864.952751	8000.361312	13.094464	-0.165829	4.816291
864.842123	8000.396639	13.099469	-0.165808	4.816302
864.579734	8000.302978	13.104474	-0.165759	4.816276
864.844924	8000.255350	13.109479	-0.165809	4.816260
864.191770	8000.248645	13.114483	-0.165687	4.816261
864.068171	8000.112687	13.119488	-0.165664	4.816222
864.495496	8000.223968	13.124493	-0.165743	4.816253
864.656965	8000.333984	13.129498	-0.165773	4.816284
864.875623	8000.362081	13.134503	-0.165814	4.816291
865.214162	8000.435754	13.139507	-0.165877	4.816311
865.673375	8000.523142	13.144512	-0.165962	4.816335
865.458518	8000.412209	13.149517	-0.165922	4.816303
865.634843	8000.454474	13.154522	-0.165955	4.816315
865.070694	8000.392939	13.159527	-0.165850	4.816300
864.926092	8000.419196	13.164531	-0.165823	4.816308
864.865461	8000.346979	13.169536	-0.165811	4.816287
865.247777	8000.503205	13.174541	-0.165883	4.816331
865.804356	8000.451965	13.179546	-0.165986	4.816313
865.301109	8000.430765	13.184551	-0.165892	4.816310
864.828389	8000.295323	13.189555	-0.165804	4.816272
864.741739	8000.171669	13.194560	-0.165788	4.816236
864.823686	8000.321792	13.199565	-0.165803	4.816280
865.171970	8000.380752	13.204570	-0.165868	4.816296
865.316041	8000.536172	13.209575	-0.165895	4.816340
865.042215	8000.416813	13.214579	-0.165844	4.816307
865.100253	8000.451781	13.219584	-0.165854	4.816317
865.169768	8000.426374	13.224589	-0.165867	4.816309
865.403244	8000.532290	13.229594	-0.165911	4.816339
865.062865	8000.325747	13.234599	-0.165847	4.816280
864.903076	8000.319872	13.239603	-0.165817	4.816279
864.833857	8000.320829	13.244608	-0.165804	4.816280
864.874357	8000.306624	13.249613	-0.165812	4.816275
865.123379	8000.402172	13.254618	-0.165858	4.816302
865.197278	8000.291833	13.259623	-0.165872	4.816269
864.807544	8000.264041	13.264627	-0.165799	4.816263
864.527054	8000.162640	13.269632	-0.165747	4.816235
864.830557	8000.246347	13.274637	-0.165803	4.816258
864.764476	8000.174041	13.279642	-0.165791	4.816237
864.769190	8000.279305	13.284647	-0.165791	4.816268
864.461768	8000.132826	13.289651	-0.165734	4.816226
864.775145	8000.269826	13.294656	-0.165792	4.816265
864.981970	8000.310474	13.299661	-0.165831	4.816276
864.605587	8000.180901	13.304666	-0.165761	4.816240
865.388989	8000.444792	13.309671	-0.165906	4.816313
864.903657	8000.275136	13.314675	-0.165816	4.816266
865.059805	8000.258619	13.319680	-0.165845	4.816260
865.286831	8000.320859	13.324685	-0.165887	4.816277
864.954662	8000.238778	13.329690	-0.165825	4.816255
864.711978	8000.159261	13.334695	-0.165780	4.816233
864.775551	8000.199633	13.339699	-0.165792	4.816244
865.097074	8000.134885	13.344704	-0.165851	4.816224
865.083533	8000.246219	13.349709	-0.165849	4.816256
865.196946	8000.193922	13.354714	-0.165870	4.816241
864.995117	8000.133153	13.359719	-0.165832	4.816224
864.984584	8000.373107	13.364723	-0.165830	4.816294
865.101455	8000.305991	13.369728	-0.165852	4.816274
864.676229	8000.163911	13.374733	-0.165772	4.816234
864.820435	8000.146132	13.379738	-0.165799	4.816228
865.186230	8000.187319	13.384743	-0.165867	4.816239
865.582368	8000.421344	13.389747	-0.165941	4.816306
865.975862	8000.377994	13.394752	-0.166014	4.816291
865.504033	8000.407263	13.399757	-0.165926	4.816302
865.693301	8000.418931	13.404762	-0.165961	4.816304
865.561271	8000.326389	13.409767	-0.165937	4.816278
865.337632	8000.404449	13.414771	-0.165895	4.816302
865.626365	8000.366780	13.419776	-0.165949	4.816289
865.496885	8000.324223	13.424781	-0.165924	4.816277
865.264035	8000.263994	13.429786	-0.165881	4.816261
865.298690	8000.258192	13.434791	-0.165887	4.816259
865.141249	8000.300172	13.439795	-0.165858	4.816272
865.000281	8000.006661	13.444800	-0.165831	4.816187
865.400899	8000.368265	13.449805	-0.165906	4.816291
865.579763	8000.388257	13.454810	-0.165939	4.816296
865.440623	8000.096897	13.459815	-0.165913	4.816211
865.323915	8000.222440	13.464819	-0.165891	4.816248
865.589694	8000.275767	13.469824	-0.165941	4.816263
865.001956	8000.157524	13.474829	-0.165831	4.816231
865.739307	8000.195379	13.479834	-0.165969	4.816238
865.477205	8000.214353	13.484839	-0.165920	4.816245
865.504224	8000.309367	13.489843	-0.165925	4.816273
865.997838	8000.239005	13.494848	-0.166016	4.816250
865.889535	8000.313687	13.499853	-0.165996	4.816272
866.039580	8000.364012	13.504858	-0.166024	4.816286
865.964198	8000.389305	13.509863	-0.166010	4.816294
865.635174	8000.396530	13.514867	-0.165949	4.816298
865.384419	8000.242494	13.519872	-0.165902	4.816254
865.168209	8000.188921	13.524877	-0.165861	4.816239
865.980646	8000.331107	13.529882	-0.166013	4.816277
865.680757	8000.352634	13.534887	-0.165957	4.816285
865.832134	8000.516679	13.539891	-0.165985	4.816332
865.943032	8000.344266	13.544896	-0.166005	4.816281
866.026244	8000.282961	13.549901	-0.166021	4.816263
865.785799	8000.296984	13.554906	-0.165976	4.816268
866.015647	8000.361399	13.559911	-0.166019	4.816286
866.149805	8000.325388	13.564915	-0.166044	4.816275
866.330356	8000.462296	13.569920	-0.166077	4.816314
865.799441	8000.276992	13.574925	-0.165978	4.816262
866.640947	8000.347417	13.579930	-0.166135	4.816279
866.263158	8000.410140	13.584935	-0.166064	4.816299
866.136117	8000.344245	13.589939	-0.166041	4.816280
865.957875	8000.371000	13.594944	-0.166007	4.816289
865.491109	8000.226092	13.599949	-0.165920	4.816249
865.712088	8000.279730	13.604954	-0.165961	4.816263
865.934462	8000.279201	13.609959	-0.166003	4.816262
866.142424	8000.473949	13.614963	-0.166041	4.816318
866.031643	8000.373261	13.619968	-0.166021	4.816289
865.781420	8000.231983	13.624973	-0.165974	4.816249
866.149419	8000.287025	13.629978	-0.166042	4.816263
866.048652	8000.319330	13.634983	-0.166024	4.816273
866.054618	8000.321547	13.639987	-0.166025	4.816274
866.217979	8000.355095	13.644992	-0.166055	4.816283
866.495075	8000.423491	13.649997	-0.166106	4.816302
866.110603	8000.374530	13.655002	-0.166035	4.816289
866.025280	8000.350776	13.660007	-0.166019	4.816283
865.692293	8000.337746	13.665011	-0.165957	4.816281
865.438806	8000.050844	13.670016	-0.165909	4.816197
865.321235	8000.168935	13.675021	-0.165887	4.816233
865.490815	8000.206834	13.680026	-0.165919	4.816243
865.502315	8000.005132	13.685031	-0.165921	4.816184
865.849590	8000.292528	13.690035	-0.165985	4.816266
865.866454	8000.115352	13.695040	-0.165988	4.816214
866.085491	8000.229525	13.700045	-0.166029	4.816247
866.053571	8000.292737	13.705050	-0.166023	4.816266
865.917813	8000.187382	13.710055	-0.165998	4.816235
865.994877	8000.190791	13.715059	-0.166012	4.816236
865.827288	8000.123156	13.720064	-0.165981	4.816217
865.429315	8000.188731	13.725069	-0.165907	4.816238
865.952852	8000.221940	13.730074	-0.166004	4.816245
866.192323	8000.156880	13.735079	-0.166048	4.816225
866.021815	8000.279398	13.740083	-0.166017	4.816262
866.172912	8000.149101	13.745088	-0.166045	4.816223
866.422907	8000.280796	13.750093	-0.166091	4.816260
866.346864	8000.225321	13.755098	-0.166077	4.816244
866.496068	8000.456275	13.760103	-0.166105	4.816311
866.562734	8000.376627	13.765107	-0.166117	4.816288
866.174453	8000.382857	13.770112	-0.166045	4.816291
866.016203	8000.236745	13.775117	-0.166015	4.816249
866.612183	8000.395497	13.780122	-0.166126	4.816293
867.011498	8000.410690	13.785127	-0.166200	4.816296
866.323351	8000.446954	13.790131	-0.166072	4.816310
866.568662	8000.315048	13.795136	-0.166118	4.816270
866.027478	8000.294274	13.800141	-0.166017	4.816266
866.413486	8000.218921	13.805146	-0.166088	4.816242
866.665939	8000.456921	13.810151	-0.166135	4.816311
866.807180	8000.388087	13.815155	-0.166162	4.816290
866.713033	8000.385437	13.820160	-0.166144	4.816290
866.497549	8000.363750	13.825165	-0.166104	4.816284
866.623549	8000.247907	13.830170	-0.166127	4.816250
866.980266	8000.502535	13.835175	-0.166194	4.816323
866.326576	8000.230159	13.840179	-0.166072	4.816246
866.418200	8000.205123	13.845184	-0.166089	4.816238
866.615449	8000.257303	13.850189	-0.166125	4.816252
866.326435	8000.270511	13.855194	-0.166071	4.816258
866.513481	8000.273641	13.860199	-0.166106	4.816258
866.899837	8000.383187	13.865203	-0.166178	4.816288
866.602539	8000.248554	13.870208	-0.166122	4.816250
866.060651	8000.249021	13.875213	-0.166021	4.816253
866.430726	8000.249906	13.880218	-0.166090	4.816251
866.500257	8000.279755	13.885223	-0.166103	4.816260
866.106873	8000.351781	13.890227	-0.166030	4.816283
866.394281	8000.123886	13.895232	-0.166083	4.816214
866.658304	8000.319573	13.900237	-0.166132	4.816271
866.658647	8000.251565	13.905242	-0.166132	4.816251
866.337609	8000.193042	13.910247	-0.166072	4.816235
866.424458	8000.334754	13.915251	-0.166089	4.816276
866.819402	8000.221297	13.920256	-0.166162	4.816241
866.578164	8000.387259	13.925261	-0.166117	4.816291
866.702996	8000.395721	13.930266	-0.166140	4.816293
866.300036	8000.149869	13.935271	-0.166065	4.816222
866.811283	8000.415586	13.940275	-0.166160	4.816298
867.100832	8000.519261	13.945280	-0.166214	4.816327
866.484760	8000.397341	13.950285	-0.166099	4.816294
866.850804	8000.411975	13.955290	-0.166167	4.816297
866.601062	8000.357834	13.960295	-0.166121	4.816282
866.577985	8000.304309	13.965299	-0.166116	4.816266
866.904959	8000.134457	13.970304	-0.166177	4.816215
866.944361	8000.359320	13.975309	-0.166184	4.816281
866.620475	8000.200863	13.980314	-0.166124	4.816236
866.852462	8000.298256	13.985319	-0.166167	4.816263
866.464796	8000.188673	13.990323	-0.166095	4.816233
866.644831	8000.308571	13.995328	-0.166128	4.816267
866.703642	8000.287235	14.000333	-0.166139	4.816261
867.096440	8000.412830	14.005338	-0.166212	4.816296
866.667767	8000.207985	14.010343	-0.166132	4.816238
866.726258	8000.263151	14.015347	-0.166143	4.816254
867.273808	8000.381779	14.020352	-0.166245	4.816286
867.110782	8000.402413	14.025357	-0.166214	4.816293
867.355044	8000.375688	14.030362	-0.166260	4.816284
867.345650	8000.320266	14.035367	-0.166258	4.816267
866.893255	8000.336045	14.040371	-0.166174	4.816274
867.087208	8000.311663	14.045376	-0.166210	4.816266
867.100586	8000.426642	14.050381	-0.166212	4.816300
866.953622	8000.199957	14.055386	-0.166185	4.816234
866.789971	8000.204642	14.060391	-0.166154	4.816236
867.343214	8000.388185	14.065395	-0.166257	4.816287
866.895493	8000.101199	14.070400	-0.166173	4.816205
866.847601	8000.371352	14.075405	-0.166165	4.816285
867.030445	8000.422230	14.080410	-0.166199	4.816299
867.020378	8000.259473	14.085415	-0.166197	4.816251
866.517296	8000.101200	14.090419	-0.166103	4.816207
866.847556	8000.159861	14.095424	-0.166164	4.816223
866.622983	8000.160337	14.100429	-0.166122	4.816224
866.485622	8000.124023	14.105434	-0.166096	4.816214
866.567235	8000.085005	14.110439	-0.166112	4.816202
867.059930	8000.277091	14.115443	-0.166203	4.816256
867.109000	8000.045196	14.120448	-0.166212	4.816188
867.170281	8000.171603	14.125453	-0.166224	4.816225
866.957973	8000.245604	14.130458	-0.166184	4.816247
867.247911	8000.207955	14.135463	-0.166238	4.816235
867.082664	8000.459140	14.140467	-0.166207	4.816310
866.910319	8000.133207	14.145472	-0.166175	4.816215
867.103190	8000.208692	14.150477	-0.166211	4.816236
867.123351	8000.227086	14.155482	-0.166214	4.816241
867.294630	8000.243766	14.160487	-0.166246	4.816245
866.939200	8000.265423	14.165491	-0.166180	4.816253
867.501972	8000.301423	14.170496	-0.166285	4.816261
867.256752	8000.302613	14.175501	-0.166239	4.816263
867.610062	8000.362728	14.180506	-0.166305	4.816279
867.322134	8000.230374	14.185511	-0.166251	4.816241
867.115774	8000.341666	14.190515	-0.166212	4.816275
866.997651	8000.108028	14.195520	-0.166190	4.816207
866.778161	8000.138342	14.200525	-0.166149	4.816217
866.829220	8000.206134	14.205530	-0.166159	4.816237
866.600292	8000.118341	14.210535	-0.166116	4.816212
867.064042	8000.256812	14.215539	-0.166202	4.816250
867.304382	8000.347971	14.220544	-0.166247	4.816276
867.155784	8000.258335	14.225549	-0.166219	4.816250
867.010393	8000.270765	14.230554	-0.166192	4.816255
867.221521	8000.309365	14.235559	-0.166231	4.816265
867.204901	8000.252760	14.240563	-0.166228	4.816248
867.295512	8000.247897	14.245568	-0.166245	4.816246
867.211649	8000.270922	14.250573	-0.166229	4.816254
867.269793	8000.185818	14.255578	-0.166240	4.816228
867.393784	8000.239958	14.260583	-0.166263	4.816244
867.023199	8000.325117	14.265587	-0.166194	4.816271
866.645491	8000.020184	14.270592	-0.166123	4.816183
866.829554	8000.201778	14.275597	-0.166158	4.816235
867.042339	8000.171336	14.280602	-0.166197	4.816225
867.129240	8000.088841	14.285607	-0.166213	4.816201
866.931229	8000.209836	14.290611	-0.166176	4.816237
866.517304	8000.162506	14.295616	-0.166099	4.816225
866.769077	8000.295296	14.300621	-0.166146	4.816263
867.059759	8000.359671	14.305626	-0.166200	4.816281
867.411137	8000.193415	14.310631	-0.166265	4.816230
867.352147	8000.280615	14.315635	-0.166254	4.816256
867.186853	8000.096127	14.320640	-0.166223	4.816202
867.518391	8000.343958	14.325645	-0.166285	4.816274
867.249252	8000.142850	14.330650	-0.166235	4.816216
867.166713	8000.131894	14.335655	-0.166219	4.816213
867.387961	8000.303491	14.340659	-0.166261	4.816262
867.514342	8000.333232	14.345664	-0.166284	4.816271
867.495020	8000.299958	14.350669	-0.166280	4.816261
867.444283	8000.200276	14.355674	-0.166271	4.816232
867.419461	8000.271047	14.360679	-0.166266	4.816253
866.948726	8000.182383	14.365683	-0.166178	4.816229
866.748979	8000.140771	14.370688	-0.166141	4.816218
866.972789	8000.148767	14.375693	-0.166182	4.816219
867.276743	8000.313250	14.380698	-0.166239	4.816266
867.335716	8000.305731	14.385703	-0.166250	4.816263
867.191053	8000.244852	14.390707	-0.166223	4.816246
867.252631	8000.076922	14.395712	-0.166234	4.816197
867.115605	8000.139435	14.400717	-0.166209	4.816216
867.393802	8000.387433	14.405722	-0.166261	4.816287
867.569956	8000.178919	14.410727	-0.166293	4.816225
867.365899	8000.200991	14.415731	-0.166255	4.816232
867.008391	8000.157794	14.420736	-0.166188	4.816222
867.567063	8000.302111	14.425741	-0.166292	4.816261
867.136871	7999.468192	14.430746	-0.166212	4.816018

867.296306	7996.341903	14.435751	-0.166239	4.815099
867.222995	7990.730255	14.440755	-0.166222	4.813450
867.028686	7984.089887	14.445760	-0.166181	4.811498
867.220035	7976.695602	14.450765	-0.166212	4.809322
867.364657	7969.103403	14.455770	-0.166234	4.807087
867.401706	7961.227823	14.460775	-0.166235	4.804768
866.824274	7953.434377	14.465779	-0.166123	4.802475
866.998519	7945.462681	14.470784	-0.166150	4.800125
866.995166	7937.513294	14.475789	-0.166144	4.797781
867.424874	7929.428318	14.480794	-0.166219	4.795394
866.818600	7921.551774	14.485799	-0.166101	4.793072
867.087071	7913.440558	14.490803	-0.166145	4.790675
867.107289	7905.493462	14.495808	-0.166144	4.788327
866.983106	7897.455284	14.500813	-0.166115	4.785952
867.546554	7889.423446	14.505818	-0.166215	4.783574
867.236289	7881.571031	14.510823	-0.166152	4.781252
866.816453	7873.481720	14.515827	-0.166068	4.778859
867.021531	7865.488316	14.520832	-0.166101	4.776490
867.091511	7857.395894	14.525837	-0.166109	4.774092
866.952999	7849.514288	14.530842	-0.166078	4.771756
866.782713	7841.459417	14.535847	-0.166041	4.769367
866.947669	7833.417124	14.540851	-0.166066	4.766980
866.710294	7825.443148	14.545856	-0.166017	4.764613
866.379911	7817.515164	14.550861	-0.165950	4.762259
866.438726	7809.483592	14.555866	-0.165956	4.759872
866.586246	7801.452896	14.560871	-0.165978	4.757483
866.527798	7793.391247	14.565875	-0.165962	4.755085
866.510071	7785.476768	14.570880	-0.165953	4.752729
866.356499	7777.422157	14.575885	-0.165919	4.750330
866.540162	7769.394297	14.580890	-0.165948	4.747938
866.590617	7761.371057	14.585895	-0.165952	4.745546
866.348288	7753.405208	14.590899	-0.165902	4.743170
866.382707	7745.412907	14.595904	-0.165903	4.740785
866.810100	7737.360750	14.600909	-0.165977	4.738380
866.116473	7729.426500	14.605914	-0.165843	4.736012
865.778797	7721.456185	14.610919	-0.165774	4.733630
865.705057	7713.392400	14.615923	-0.165755	4.731219
866.461814	7705.295867	14.620928	-0.165891	4.728795
866.227063	7697.380535	14.625933	-0.165842	4.726426
865.991750	7689.326485	14.630938	-0.165793	4.724015
866.409599	7681.426277	14.635943	-0.165865	4.721646
866.028604	7673.362508	14.640947	-0.165789	4.719230
866.878655	7665.392718	14.645952	-0.165942	4.716837
866.674773	7657.310649	14.650957	-0.165899	4.714412
866.168681	7649.434089	14.655962	-0.165799	4.712049
866.218914	7641.339650	14.660967	-0.165803	4.709617
866.034838	7633.347237	14.665971	-0.165764	4.707215
866.274020	7625.295790	14.670976	-0.165803	4.704793
866.407671	7617.350322	14.675981	-0.165823	4.702403
866.076305	7609.328751	14.680986	-0.165755	4.699989
865.934084	7601.384280	14.685991	-0.165724	4.697596
865.947217	7593.290651	14.690995	-0.165721	4.695157
865.961532	7585.353423	14.696000	-0.165718	4.692764
865.641290	7577.342547	14.701005	-0.165653	4.690349
865.558626	7569.298123	14.706010	-0.165633	4.687921
865.800443	7561.332234	14.711015	-0.165672	4.685515
865.554430	7553.326157	14.716019	-0.165621	4.683097
866.295996	7545.303091	14.721024	-0.165754	4.680670
865.504284	7537.368366	14.726029	-0.165601	4.678272
865.798653	7529.358166	14.731034	-0.165651	4.675848
865.727910	7521.321283	14.736039	-0.165632	4.673415
865.348481	7513.259285	14.741043	-0.165556	4.670973
865.575365	7505.263220	14.746048	-0.165593	4.668550
865.434944	7497.298390	14.751053	-0.165562	4.666135
865.047019	7489.268776	14.756058	-0.165484	4.663700
865.167643	7481.347413	14.761063	-0.165501	4.661295
865.026591	7473.263603	14.766067	-0.165470	4.658840
864.653088	7465.394853	14.771072	-0.165395	4.656450
864.772744	7457.301044	14.776077	-0.165412	4.653989
865.104524	7449.275806	14.781082	-0.165468	4.651547
864.633875	7441.317771	14.786087	-0.165376	4.649126
864.877638	7433.349784	14.791091	-0.165416	4.646700
865.046804	7425.317025	14.796096	-0.165442	4.644252
864.656221	7417.373020	14.801101	-0.165364	4.641831
864.174773	7409.296990	14.806106	-0.165269	4.639368
864.301300	7401.365877	14.811111	-0.165287	4.636948
864.240043	7393.298432	14.816115	-0.165270	4.634485
863.920154	7385.441250	14.821120	-0.165206	4.632085
863.717245	7377.350505	14.826125	-0.165163	4.629613
863.527768	7369.329515	14.831130	-0.165122	4.627160
864.027189	7361.252474	14.836135	-0.165210	4.624689
863.534679	7353.342731	14.841139	-0.165113	4.622268
864.334906	7345.236597	14.846144	-0.165256	4.619785
863.885329	7337.321163	14.851149	-0.165167	4.617359
863.844363	7329.279939	14.856154	-0.165154	4.614894
864.301614	7321.289950	14.861159	-0.165234	4.612443
864.370177	7313.227760	14.866163	-0.165242	4.609968
864.365634	7305.244088	14.871168	-0.165235	4.607517
864.071944	7297.266812	14.876173	-0.165175	4.605065
864.108873	7289.350577	14.881178	-0.165177	4.602632
863.690947	7281.344495	14.886183	-0.165094	4.600169
863.152704	7273.372397	14.891187	-0.164988	4.597716
863.410616	7265.328855	14.896192	-0.165031	4.595239
863.217577	7257.322580	14.901197	-0.164990	4.592772
862.812928	7249.280514	14.906202	-0.164909	4.590293
862.841905	7241.285725	14.911207	-0.164909	4.587827
862.904340	7233.193012	14.916211	-0.164916	4.585330
862.626035	7225.296471	14.921216	-0.164859	4.582892
862.511833	7217.280609	14.926221	-0.164832	4.580415
862.625724	7209.232209	14.931226	-0.164848	4.577928
862.345715	7201.298213	14.936231	-0.164790	4.575474
862.241021	7193.230901	14.941235	-0.164766	4.572978
862.393032	7185.189426	14.946240	-0.164789	4.570488
862.397780	7177.201131	14.951245	-0.164784	4.568014
862.207661	7169.213824	14.956250	-0.164743	4.565538
862.664134	7161.221504	14.961255	-0.164823	4.563060
862.599428	7153.241413	14.966259	-0.164806	4.560584
862.410121	7145.291332	14.971264	-0.164765	4.558116
862.187366	7137.227211	14.976269	-0.164719	4.555610
862.354393	7129.207058	14.981274	-0.164744	4.553118
862.767278	7121.198124	14.986279	-0.164816	4.550628
861.939007	7113.229540	14.991283	-0.164656	4.548148
862.235781	7105.145655	14.996288	-0.164706	4.545632
862.057020	7097.206920	15.001293	-0.164668	4.543159
862.147631	7089.162955	15.006298	-0.164679	4.540652
861.928586	7081.236258	15.011303	-0.164633	4.538180
861.993726	7073.164255	15.016307	-0.164640	4.535662
861.958734	7065.242302	15.021312	-0.164628	4.533189
861.820735	7057.154451	15.026317	-0.164597	4.530663
862.065695	7049.113661	15.031322	-0.164637	4.528151
862.263070	7041.150430	15.036327	-0.164669	4.525661
861.799776	7033.201993	15.041331	-0.164577	4.523173
861.811764	7025.240833	15.046336	-0.164574	4.520681
862.020840	7017.197942	15.051341	-0.164608	4.518163
861.990019	7009.132350	15.056346	-0.164597	4.515635
861.726568	7001.213417	15.061351	-0.164543	4.513152
862.068296	6993.100243	15.066355	-0.164601	4.510607
862.023973	6985.164630	15.071360	-0.164587	4.508116
861.407209	6977.171523	15.076365	-0.164467	4.505604
861.290931	6969.150136	15.081370	-0.164440	4.503083
861.692913	6961.172534	15.086375	-0.164510	4.500576
861.665683	6953.098816	15.091379	-0.164499	4.498036
861.580089	6945.128363	15.096384	-0.164478	4.495527
861.337479	6937.138073	15.101389	-0.164428	4.493010
861.482864	6929.073468	15.106394	-0.164449	4.490469
861.357785	6921.156519	15.111399	-0.164421	4.487972
860.936073	6913.124246	15.116403	-0.164337	4.485437
861.317796	6905.126286	15.121408	-0.164403	4.482913
861.399867	6897.097181	15.126413	-0.164413	4.480377
861.062759	6889.114452	15.131418	-0.164345	4.477854
861.375484	6881.084130	15.136423	-0.164398	4.475315
861.013538	6873.087175	15.141427	-0.164325	4.472784
861.362114	6865.068419	15.146432	-0.164385	4.470247
861.456420	6857.076616	15.151437	-0.164397	4.467716
861.378180	6849.055808	15.156442	-0.164377	4.465174
861.204570	6841.127317	15.161447	-0.164339	4.462659
860.888104	6833.130280	15.166451	-0.164275	4.460120
860.798238	6825.167682	15.171456	-0.164253	4.457592
861.058442	6817.038383	15.176461	-0.164296	4.455011
860.775673	6809.069625	15.181466	-0.164238	4.452477
860.545475	6801.096036	15.186471	-0.164190	4.449940
860.227031	6793.125268	15.191475	-0.164125	4.447403
860.324088	6785.050911	15.196480	-0.164138	4.444832
860.269013	6777.118383	15.201485	-0.164123	4.442305
860.195066	6769.083920	15.206490	-0.164104	4.439744
859.916164	6761.147896	15.211495	-0.164046	4.437212
860.423240	6752.994546	15.216499	-0.164135	4.434612
860.351733	6745.056123	15.221504	-0.164117	4.432077
860.164346	6737.036959	15.226509	-0.164077	4.429514
860.125630	6729.026262	15.231514	-0.164064	4.426953
860.437344	6721.000537	15.236519	-0.164117	4.424387
859.897135	6713.065915	15.241523	-0.164011	4.421845
859.947407	6705.020125	15.246528	-0.164015	4.419269
860.017663	6697.028393	15.251533	-0.164023	4.416709
860.127183	6688.986163	15.256538	-0.164038	4.414131
860.341312	6680.996605	15.261543	-0.164072	4.411569
859.681606	6673.011618	15.266547	-0.163944	4.409003
859.802213	6665.050334	15.271552	-0.163962	4.406446
859.750960	6657.013822	15.276557	-0.163947	4.403864
859.788311	6649.036918	15.281562	-0.163948	4.401299
859.694997	6641.041574	15.286567	-0.163926	4.398726
859.584476	6633.022153	15.291571	-0.163900	4.396144
860.051960	6624.967773	15.296576	-0.163981	4.393552
859.525941	6617.081034	15.301581	-0.163878	4.391007
859.745493	6608.949187	15.306586	-0.163914	4.388386
859.447609	6600.957801	15.311591	-0.163853	4.385806
859.475607	6592.973263	15.316595	-0.163853	4.383228
859.811527	6584.992789	15.321600	-0.163910	4.380652
859.571830	6577.023341	15.326605	-0.163860	4.378074
859.326414	6569.011512	15.331610	-0.163809	4.375481
859.478849	6561.013645	15.336615	-0.163832	4.372894
859.313782	6552.964654	15.341619	-0.163796	4.370286
859.626107	6544.958808	15.346624	-0.163849	4.367694
859.486919	6536.970946	15.351629	-0.163818	4.365103
859.537985	6528.997726	15.356634	-0.163822	4.362517
859.338764	6521.006167	15.361639	-0.163780	4.359922
858.951025	6513.073096	15.366643	-0.163702	4.357343
859.080369	6505.010823	15.371648	-0.163721	4.354723
859.108597	6496.975523	15.376653	-0.163721	4.352111
859.061975	6488.903383	15.381658	-0.163707	4.349484
859.005671	6480.992598	15.386663	-0.163691	4.346908
858.510922	6472.989162	15.391667	-0.163594	4.344297
858.715916	6465.034693	15.396672	-0.163627	4.341705
858.690762	6456.996881	15.401677	-0.163617	4.339084
858.809223	6448.959966	15.406682	-0.163633	4.336461
858.913355	6440.975008	15.411687	-0.163648	4.333855
858.533680	6432.998506	15.416691	-0.163572	4.331246
859.001173	6424.926552	15.421696	-0.163653	4.328610
859.378490	6416.885154	15.426701	-0.163718	4.325982
858.737738	6408.993908	15.431706	-0.163594	4.323394
858.871474	6401.038993	15.436711	-0.163613	4.320789
858.593944	6393.070430	15.441715	-0.163556	4.318175
858.189869	6385.103962	15.446720	-0.163476	4.315560
858.096607	6377.093560	15.451725	-0.163453	4.312930
858.142634	6369.063024	15.456730	-0.163456	4.310294
858.538829	6361.032120	15.461735	-0.163525	4.307658
858.484146	6352.972854	15.466739	-0.163509	4.305008
858.684336	6344.968547	15.471744	-0.163541	4.302377
858.527907	6336.996507	15.476749	-0.163507	4.299751
858.039019	6329.025058	15.481754	-0.163411	4.297122
858.294287	6320.988625	15.486759	-0.163453	4.294476
858.159033	6312.999689	15.491763	-0.163422	4.291840
857.717029	6304.986369	15.496768	-0.163335	4.289192
857.668192	6297.023277	15.501773	-0.163320	4.286562
858.013634	6288.941902	15.506778	-0.163379	4.283895
857.774381	6281.100102	15.511783	-0.163329	4.281301
857.329453	6273.069289	15.516787	-0.163241	4.278641
857.455595	6265.023422	15.521792	-0.163259	4.275979
857.324681	6257.007040	15.526797	-0.163230	4.273322
857.140422	6248.977311	15.531802	-0.163190	4.270660
857.248384	6240.961039	15.536807	-0.163205	4.268002
857.824239	6232.887562	15.541811	-0.163307	4.265328
857.561360	6224.954892	15.546816	-0.163253	4.262692
857.365841	6216.998204	15.551821	-0.163211	4.260047
857.418421	6208.981666	15.556826	-0.163215	4.257382
857.550952	6200.982041	15.561831	-0.163235	4.254722
857.392518	6192.969059	15.566835	-0.163200	4.252053
857.240102	6184.988188	15.571840	-0.163166	4.249394
856.885695	6177.067606	15.576845	-0.163095	4.246751
856.553483	6169.003626	15.581850	-0.163028	4.244058
856.690720	6161.111296	15.586855	-0.163048	4.241426
856.816064	6152.979272	15.591859	-0.163066	4.238712
856.669723	6145.014267	15.596864	-0.163034	4.236049
856.838187	6136.942635	15.601869	-0.163060	4.233352
856.792501	6128.962491	15.606874	-0.163046	4.230681
857.087436	6120.970062	15.611879	-0.163095	4.228009
856.997961	6112.925799	15.616883	-0.163073	4.225313
856.898084	6105.008995	15.621888	-0.163050	4.222659
856.850450	6097.031465	15.626893	-0.163035	4.219982
856.985083	6088.984772	15.631898	-0.163055	4.217283
856.526862	6081.024174	15.636903	-0.162965	4.214605
856.588221	6072.999267	15.641907	-0.162971	4.211909
856.773941	6064.922796	15.646912	-0.163000	4.209195
856.719390	6057.005371	15.651917	-0.162985	4.206530
856.683187	6048.965435	15.656922	-0.162972	4.203823
856.066892	6041.077442	15.661927	-0.162852	4.201159
855.788436	6033.059199	15.666931	-0.162795	4.198453
855.731483	6025.034672	15.671936	-0.162779	4.195745
855.835362	6016.972370	15.676941	-0.162793	4.193024
856.112522	6008.848779	15.681946	-0.162840	4.190283
855.877999	6000.972977	15.686951	-0.162791	4.187619
855.850031	5992.915710	15.691955	-0.162780	4.184893
855.787227	5984.960742	15.696960	-0.162763	4.182200
855.936403	5976.921091	15.701965	-0.162786	4.179479
855.887724	5968.957569	15.706970	-0.162771	4.176780
855.916308	5960.940535	15.711975	-0.162771	4.174061
855.875080	5952.943911	15.716979	-0.162758	4.171347
856.173561	5944.836408	15.721984	-0.162809	4.168598
855.927817	5936.993046	15.726989	-0.162758	4.165930
855.843355	5928.968541	15.731994	-0.162737	4.163201
856.448272	5920.900272	15.736999	-0.162844	4.160463
856.004928	5912.985591	15.742003	-0.162756	4.157763
856.419455	5904.926795	15.747008	-0.162828	4.155023
856.113659	5896.995052	15.752013	-0.162766	4.152315
856.083838	5888.883372	15.757018	-0.162755	4.149548
855.942683	5880.978504	15.762023	-0.162723	4.146848
856.050905	5872.902886	15.767027	-0.162738	4.144091
856.013358	5865.007591	15.772032	-0.162726	4.141392
855.665696	5857.016225	15.777037	-0.162656	4.138655
855.388827	5848.978530	15.782042	-0.162599	4.135901
855.213990	5840.996418	15.787047	-0.162561	4.133165
855.046007	5832.972069	15.792051	-0.162524	4.130413
855.251301	5824.916859	15.797056	-0.162557	4.127653
855.308863	5816.914180	15.802061	-0.162563	4.124907
855.415342	5808.962281	15.807066	-0.162577	4.122178
855.550771	5800.972766	15.812071	-0.162597	4.119435
855.170337	5793.018523	15.817075	-0.162521	4.116695
855.283273	5784.943433	15.822080	-0.162537	4.113918
855.081366	5777.000657	15.827085	-0.162494	4.111180
854.974512	5768.936494	15.832090	-0.162469	4.108400
855.005211	5760.944151	15.837095	-0.162469	4.105645
854.504505	5753.010838	15.842099	-0.162371	4.102902
854.774055	5744.980394	15.847104	-0.162416	4.100133
854.569591	5737.064715	15.852109	-0.162372	4.097395
854.388575	5728.976570	15.857114	-0.162333	4.094597
854.402122	5721.019107	15.862119	-0.162330	4.091844
854.311597	5712.975495	15.867123	-0.162308	4.089058
854.558666	5704.990849	15.872128	-0.162349	4.086296
854.328359	5696.973587	15.877133	-0.162301	4.083513
854.393393	5688.991591	15.882138	-0.162308	4.080745
854.354157	5680.994863	15.887143	-0.162295	4.077969
854.378288	5672.932788	15.892147	-0.162294	4.075169
854.275603	5665.025002	15.897152	-0.162270	4.072419
854.116053	5657.016336	15.902157	-0.162235	4.069631
854.089985	5648.954919	15.907162	-0.162225	4.066824
854.302471	5640.910869	15.912167	-0.162259	4.064026
854.120710	5633.005715	15.917171	-0.162220	4.061268
853.903039	5625.001013	15.922176	-0.162174	4.058472
854.067566	5616.991494	15.927181	-0.162199	4.055679
854.268537	5608.943922	15.932186	-0.162231	4.052871
853.741545	5601.035798	15.937191	-0.162128	4.050099
853.573412	5593.009414	15.942195	-0.162091	4.047290
853.516160	5584.980446	15.947200	-0.162075	4.044479
853.550153	5577.049466	15.952205	-0.162076	4.041701
853.403928	5568.976653	15.957210	-0.162044	4.038870
853.637284	5561.002812	15.962215	-0.162082	4.036076
853.728939	5552.915102	15.967219	-0.162094	4.033239
853.503136	5544.898266	15.972224	-0.162046	4.030420
853.377985	5536.927183	15.977229	-0.162018	4.027616
853.261477	5528.911644	15.982234	-0.161991	4.024795
853.297359	5520.980249	15.987239	-0.161992	4.022004
853.712092	5512.862292	15.992243	-0.162064	4.019151
853.694066	5504.943432	15.997248	-0.162055	4.016360
853.615020	5496.973508	16.002253	-0.162035	4.013548
853.824173	5488.878801	16.007258	-0.162069	4.010694
853.900211	5480.926488	16.012263	-0.162078	4.007886
853.568033	5472.972419	16.017267	-0.162011	4.005070
853.579115	5465.015694	16.022272	-0.162008	4.002255
853.028100	5457.039731	16.027277	-0.161900	3.999423
853.261352	5449.035798	16.032282	-0.161938	3.996592
853.299256	5441.005856	16.037287	-0.161940	3.993746
853.198897	5432.987083	16.042291	-0.161916	3.990900
853.046786	5424.979098	16.047296	-0.161882	3.988055
852.969344	5417.014742	16.052301	-0.161862	3.985225
852.874407	5409.048995	16.057306	-0.161839	3.982392
852.827477	5401.020051	16.062311	-0.161825	3.979535
852.797340	5393.058359	16.067315	-0.161814	3.976700
852.572505	5385.034419	16.072320	-0.161767	3.973838
853.011085	5376.959679	16.077325	-0.161843	3.970966
852.783637	5368.979011	16.082330	-0.161796	3.968115
853.059761	5360.971489	16.087335	-0.161842	3.965261
852.604680	5353.071805	16.092339	-0.161752	3.962431
852.477199	5345.062745	16.097344	-0.161723	3.959565
852.859872	5337.062895	16.102349	-0.161789	3.956710
852.529055	5329.034297	16.107354	-0.161722	3.953829
852.530993	5321.010354	16.112359	-0.161717	3.950954
852.823166	5312.953744	16.117363	-0.161766	3.948071
852.648091	5304.979688	16.122368	-0.161728	3.945206
852.882124	5297.007052	16.127373	-0.161766	3.942347
853.255759	5288.924666	16.132378	-0.161831	3.939449
853.169803	5281.042659	16.137383	-0.161809	3.936613
852.452545	5273.063337	16.142387	-0.161671	3.933729
852.266360	5265.074946	16.147392	-0.161631	3.930849
851.907609	5257.108069	16.152397	-0.161559	3.927971
851.874333	5249.025261	16.157402	-0.161547	3.925055
852.278330	5241.025835	16.162407	-0.161617	3.922175
852.403876	5232.985753	16.167411	-0.161635	3.919273
852.213907	5225.075550	16.172416	-0.161594	3.916410
852.272111	5217.023961	16.177421	-0.161600	3.913498
852.030806	5209.035081	16.182426	-0.161550	3.910602
852.247677	5201.055356	16.187431	-0.161585	3.907715
851.941493	5193.055092	16.192435	-0.161522	3.904809
851.854820	5185.093408	16.197440	-0.161501	3.901918
851.744263	5177.099373	16.202445	-0.161475	3.899014
851.611512	5169.068708	16.207450	-0.161445	3.896093
851.736012	5161.058102	16.212455	-0.161463	3.893182
851.437885	5153.061106	16.217459	-0.161402	3.890266
850.968543	5145.134128	16.222464	-0.161309	3.887370
850.945968	5137.062849	16.227469	-0.161300	3.884428
851.107303	5129.082032	16.232474	-0.161325	3.881520
851.411253	5121.073868	16.237479	-0.161376	3.878603
851.370878	5113.043074	16.242483	-0.161363	3.875669
851.185367	5104.981804	16.247488	-0.161323	3.872718
851.297078	5096.942278	16.252493	-0.161339	3.869779
851.347821	5088.926613	16.257498	-0.161343	3.866845
851.122891	5080.989928	16.262503	-0.161296	3.863933
850.749544	5073.136370	16.267507	-0.161221	3.861046
850.776194	5065.043274	16.272512	-0.161221	3.858076
850.693817	5057.096665	16.277517	-0.161200	3.855156
850.812220	5049.046542	16.282522	-0.161217	3.852200
850.742033	5041.045238	16.287527	-0.161198	3.849256
850.839261	5033.056901	16.292531	-0.161211	3.846317
850.675647	5025.056983	16.297536	-0.161175	3.843367
850.864415	5017.082512	16.302541	-0.161205	3.840431
850.606347	5009.092625	16.307546	-0.161152	3.837478
850.426358	5001.100382	16.312551	-0.161113	3.834523
850.384354	4993.131077	16.317555	-0.161100	3.831578
850.380274	4985.089821	16.322560	-0.161094	3.828604
850.130878	4977.137089	16.327565	-0.161042	3.825656
850.364273	4969.092249	16.332570	-0.161080	3.822681
850.345609	4961.146324	16.337575	-0.161072	3.819735
850.181847	4953.158519	16.342579	-0.161036	3.816769
850.312138	4945.065043	16.347584	-0.161055	3.813767
850.432219	4937.104478	16.352589	-0.161072	3.810812
850.860428	4929.013798	16.357594	-0.161146	3.807813
850.585553	4921.080156	16.362599	-0.161090	3.804855
850.568676	4913.102526	16.367603	-0.161081	3.801884
850.289632	4905.147365	16.372608	-0.161024	3.798913
850.116064	4897.221631	16.377613	-0.160986	3.795953
850.249245	4889.095934	16.382618	-0.161006	3.792923
850.349226	4881.084740	16.387623	-0.161019	3.789932
850.159215	4873.141312	16.392627	-0.160979	3.786958
850.390506	4865.038963	16.397632	-0.161016	3.783932
849.983910	4857.223691	16.402637	-0.160935	3.780996
850.122162	4849.116317	16.407642	-0.160956	3.777961
849.788894	4841.174439	16.412647	-0.160888	3.774975
849.442178	4833.212374	16.417651	-0.160819	3.771978
849.448440	4825.135707	16.422656	-0.160814	3.768944
849.471241	4817.184073	16.427661	-0.160813	3.765955
849.049551	4809.190391	16.432666	-0.160730	3.762938
849.236637	4801.157763	16.437671	-0.160759	3.759917
849.476406	4793.163060	16.442675	-0.160798	3.756910
849.575654	4785.091473	16.447680	-0.160812	3.753868
849.206609	4777.221503	16.452685	-0.160738	3.750888
849.695517	4769.108993	16.457690	-0.160823	3.747835
849.378731	4761.158635	16.462695	-0.160759	3.744822
849.415609	4753.167195	16.467699	-0.160761	3.741799
849.460700	4745.164385	16.472704	-0.160764	3.738769
849.528688	4737.206958	16.477709	-0.160771	3.735755
849.416966	4729.141366	16.482714	-0.160745	3.732693
849.075222	4721.255631	16.487719	-0.160676	3.729691
849.214977	4713.212835	16.492723	-0.160697	3.726638
848.817963	4705.250074	16.497728	-0.160618	3.723601
848.869873	4697.275220	16.502733	-0.160622	3.720567
849.464735	4689.175458	16.507738	-0.160727	3.717497
848.964831	4681.282505	16.512743	-0.160629	3.714476
849.073549	4673.199993	16.517747	-0.160644	3.711395
848.788897	4665.230446	16.522752	-0.160586	3.708345
848.931965	4657.199076	16.527757	-0.160607	3.705280
848.638836	4649.226271	16.532762	-0.160547	3.702223
848.781780	4641.215491	16.537767	-0.160568	3.699161
848.717370	4633.240307	16.542771	-0.160551	3.696104
848.784316	4625.206175	16.547776	-0.160558	3.693025
848.680633	4617.254176	16.552781	-0.160534	3.689971
848.853658	4609.211761	16.557786	-0.160561	3.686887
848.461150	4601.293752	16.562791	-0.160482	3.683834
848.020419	4593.336198	16.567795	-0.160395	3.680762
848.153665	4585.281686	16.572800	-0.160414	3.677664
848.376136	4577.214192	16.577805	-0.160450	3.674561
848.241461	4569.299485	16.582810	-0.160420	3.671505
848.455567	4561.256473	16.587815	-0.160455	3.668406
848.147327	4553.274679	16.592819	-0.160392	3.665315
848.315187	4545.270885	16.597824	-0.160418	3.662225
848.008475	4537.331681	16.602829	-0.160356	3.659145
848.131571	4529.287963	16.607834	-0.160373	3.656032
848.095536	4521.319836	16.612839	-0.160361	3.652943
847.703814	4513.311948	16.617843	-0.160283	3.649826
847.441892	4505.405079	16.622848	-0.160229	3.646749
847.696339	4497.318609	16.627853	-0.160271	3.643613
847.324168	4489.353514	16.632858	-0.160196	3.640505
847.474016	4481.376211	16.637863	-0.160219	3.637404
847.299470	4473.340790	16.642867	-0.160181	3.634268
847.314773	4465.360837	16.647872	-0.160179	3.631157
847.214788	4457.370158	16.652877	-0.160155	3.628036
847.276211	4449.312031	16.657882	-0.160161	3.624890
847.369846	4441.362391	16.662887	-0.160173	3.621784
847.138146	4433.353837	16.667891	-0.160125	3.618644
846.837117	4425.407422	16.672896	-0.160063	3.615524
847.190885	4417.372449	16.677901	-0.160124	3.612384
846.988057	4409.333576	16.682906	-0.160081	3.609224
847.634393	4401.302791	16.687911	-0.160196	3.606089
847.301281	4393.361087	16.692915	-0.160128	3.602958
847.089859	4385.412206	16.697920	-0.160084	3.599826
847.057249	4377.453594	16.702925	-0.160072	3.596692
847.071333	4369.402762	16.707930	-0.160070	3.593520
847.130623	4361.415132	16.712935	-0.160075	3.590371
846.868975	4353.444982	16.717939	-0.160021	3.587218
846.825948	4345.393490	16.722944	-0.160008	3.584035
846.833833	4337.482009	16.727949	-0.160004	3.580907
846.951239	4329.402325	16.732954	-0.160021	3.577713
846.717387	4321.484607	16.737959	-0.159972	3.574569
846.493769	4313.517335	16.742963	-0.159925	3.571404
846.798443	4305.406857	16.747968	-0.159977	3.568194
846.362119	4297.477409	16.752973	-0.159890	3.565032
846.158546	4289.516859	16.757978	-0.159847	3.561861
846.482424	4281.473560	16.762983	-0.159902	3.558670
846.306348	4273.501000	16.767987	-0.159864	3.555490
846.219693	4265.459347	16.772992	-0.159842	3.552282
846.070563	4257.467980	16.777997	-0.159809	3.549089
845.948992	4249.431810	16.783002	-0.159781	3.545876
846.088766	4241.443541	16.788007	-0.159802	3.542687
846.207581	4233.455399	16.793011	-0.159819	3.539495
845.960957	4225.519051	16.798016	-0.159768	3.536310
845.609230	4217.536390	16.803021	-0.159697	3.533100
845.880992	4209.443215	16.808026	-0.159742	3.529861
846.098865	4201.461690	16.813031	-0.159777	3.526663
845.974628	4193.469055	16.818035	-0.159749	3.523447
845.730095	4185.534062	16.823040	-0.159698	3.520248
845.541991	4177.644717	16.828045	-0.159658	3.517065
845.370731	4169.598702	16.833050	-0.159621	3.513817
845.271729	4161.626608	16.838055	-0.159597	3.510599
845.122502	4153.617824	16.843059	-0.159564	3.507361
845.487169	4145.492680	16.848064	-0.159626	3.504088
845.489699	4137.584279	16.853069	-0.159622	3.500890
845.207559	4129.600365	16.858074	-0.159564	3.497648
845.042289	4121.609510	16.863079	-0.159528	3.494405
845.110538	4113.577179	16.868083	-0.159535	3.491149
844.933885	4105.589901	16.873088	-0.159497	3.487900
844.873277	4097.606435	16.878093	-0.159480	3.484654
844.900145	4089.660395	16.883098	-0.159480	3.481423
845.064870	4081.654154	16.888103	-0.159505	3.478169
844.850215	4073.656181	16.893107	-0.159460	3.474902
844.624350	4065.672075	16.898112	-0.159413	3.471638
844.604915	4057.631828	16.903117	-0.159404	3.468355
844.550432	4049.605051	16.908122	-0.159388	3.465073
844.891869	4041.619955	16.913127	-0.159447	3.461817
844.742117	4033.626592	16.918131	-0.159414	3.458540
844.373212	4025.686607	16.923136	-0.159340	3.455273
844.882971	4017.619860	16.928141	-0.159429	3.451981
844.874947	4009.612891	16.933146	-0.159422	3.448693
844.629367	4001.692713	16.938151	-0.159371	3.445429
844.425199	3993.737366	16.943155	-0.159328	3.442150
844.872614	3985.638367	16.948160	-0.159406	3.438829
844.622981	3977.753526	16.953165	-0.159354	3.435571
844.435737	3969.753218	16.958170	-0.159314	3.432264
844.518328	3961.709968	16.963175	-0.159324	3.428945
844.503809	3953.747339	16.968179	-0.159316	3.425653
844.087792	3945.794396	16.973184	-0.159233	3.422348
844.174108	3937.750013	16.978189	-0.159244	3.419019
844.134883	3929.795282	16.983194	-0.159232	3.415719
844.192698	3921.765048	16.988199	-0.159237	3.412389
844.063076	3913.753649	16.993203	-0.159208	3.409056
844.125359	3905.779246	16.998208	-0.159214	3.405743
844.614419	3897.743330	17.003213	-0.159300	3.402415
844.635090	3889.741384	17.008218	-0.159298	3.399082
844.509759	3881.851524	17.013223	-0.159270	3.395787
844.133119	3873.861118	17.018227	-0.159194	3.392439
844.068116	3865.801083	17.023232	-0.159177	3.389068
843.986128	3857.848263	17.028237	-0.159156	3.385739
843.892622	3849.847637	17.033242	-0.159134	3.382386
843.986981	3841.810813	17.038247	-0.159146	3.379021
843.706631	3833.884380	17.043251	-0.159088	3.375686
843.678942	3825.882033	17.048256	-0.159078	3.372325
843.657556	3817.860421	17.053261	-0.159069	3.368952
843.297744	3809.897249	17.058266	-0.158996	3.365588
843.089645	3801.972204	17.063271	-0.158952	3.362243
843.658918	3793.833075	17.068275	-0.159053	3.358832
843.454903	3785.908879	17.073280	-0.159010	3.355480
843.446007	3777.926408	17.078285	-0.159003	3.352107
843.296721	3769.934585	17.083290	-0.158970	3.348722
843.476438	3761.911397	17.088295	-0.158998	3.345332
843.686865	3753.901697	17.093299	-0.159032	3.341946
843.131170	3746.005591	17.098304	-0.158923	3.338576
843.464340	3737.987393	17.103309	-0.158980	3.335183
843.125065	3729.980107	17.108314	-0.158911	3.331767
842.953129	3722.022295	17.113319	-0.158874	3.328375
843.194087	3713.957356	17.118323	-0.158913	3.324949
843.249058	3706.006251	17.123328	-0.158918	3.321561
843.150073	3698.059249	17.128333	-0.158895	3.318165
843.186393	3690.002587	17.133338	-0.158896	3.314725
842.874579	3682.083571	17.138343	-0.158833	3.311326
842.905474	3674.020008	17.143347	-0.158833	3.307875
842.871511	3666.028860	17.148352	-0.158822	3.304449
842.529416	3658.153466	17.153357	-0.158753	3.301057
842.446304	3650.147695	17.158362	-0.158732	3.297616
842.465167	3642.108544	17.163367	-0.158730	3.294160
842.271791	3634.123673	17.168371	-0.158689	3.290716
842.196633	3626.105496	17.173376	-0.158669	3.287259
842.057058	3618.138494	17.178381	-0.158638	3.283818
842.360664	3610.108853	17.183386	-0.158689	3.280363
842.318517	3602.135395	17.188391	-0.158676	3.276915
842.245639	3594.124815	17.193395	-0.158657	3.273447
842.193783	3586.125898	17.198400	-0.158642	3.269980
842.484997	3578.118670	17.203405	-0.158691	3.266520
842.157941	3570.168259	17.208410	-0.158625	3.263057
841.816840	3562.248564	17.213415	-0.158556	3.259602
841.720539	3554.253318	17.218419	-0.158533	3.256121
841.429604	3546.282386	17.223424	-0.158474	3.252638
841.441259	3538.251503	17.228429	-0.158471	3.249138
841.266502	3530.276486	17.233434	-0.158433	3.245651
841.400745	3522.281590	17.238439	-0.158452	3.242164
841.552851	3514.227934	17.243443	-0.158475	3.238649
841.790873	3506.238421	17.248448	-0.158514	3.235161
841.751736	3498.288156	17.253453	-0.158502	3.231675
841.836585	3490.228969	17.258458	-0.158512	3.228143
842.116085	3482.185264	17.263463	-0.158559	3.224622
842.059424	3474.271783	17.268467	-0.158543	3.221140
841.607284	3466.340148	17.273472	-0.158454	3.217630
841.492410	3458.336859	17.278477	-0.158427	3.214099
841.515194	3450.345033	17.283482	-0.158426	3.210575
841.461973	3442.376915	17.288487	-0.158411	3.207054
841.090375	3434.367908	17.293491	-0.158336	3.203497
840.744092	3426.431855	17.298496	-0.158267	3.199970
841.032454	3418.431128	17.303501	-0.158315	3.196437
841.207102	3410.344402	17.308506	-0.158342	3.192858
841.054156	3402.380084	17.313511	-0.158308	3.189315
841.137738	3394.413345	17.318515	-0.158319	3.185776
840.952506	3386.436965	17.323520	-0.158279	3.182219
840.745880	3378.480056	17.328525	-0.158235	3.178665
840.802670	3370.473273	17.333530	-0.158241	3.175095
840.634606	3362.502001	17.338535	-0.158204	3.171529
840.705912	3354.479707	17.343539	-0.158212	3.167945
840.536298	3346.472311	17.348544	-0.158175	3.164354
840.636384	3338.565663	17.353549	-0.158188	3.160815
840.318696	3330.573415	17.358554	-0.158124	3.157216
840.204181	3322.587365	17.363559	-0.158097	3.153625
840.763082	3314.477556	17.368563	-0.158196	3.150003
840.068683	3306.614199	17.373568	-0.158062	3.146433
840.450395	3298.529547	17.378573	-0.158127	3.142806
840.299856	3290.566365	17.383578	-0.158094	3.139207
840.845036	3282.514377	17.388583	-0.158190	3.135594
840.399040	3274.608937	17.393587	-0.158102	3.132000
840.127659	3266.634936	17.398592	-0.158046	3.128377
840.339125	3258.612978	17.403597	-0.158080	3.124751
840.296064	3250.661176	17.408602	-0.158067	3.121141
840.479905	3242.627417	17.413607	-0.158096	3.117499
840.315477	3234.695184	17.418611	-0.158060	3.113884
840.605182	3226.640017	17.423616	-0.158108	3.110229
840.237913	3218.741834	17.428621	-0.158035	3.106611
840.398224	3210.679316	17.433626	-0.158059	3.102939
840.227559	3202.747486	17.438631	-0.158022	3.099306
840.332375	3194.746939	17.443635	-0.158036	3.095651
840.476369	3186.705533	17.448640	-0.158058	3.091974
840.303426	3178.751128	17.453645	-0.158021	3.088318
840.201110	3170.767845	17.458650	-0.157996	3.084648
839.428206	3162.953550	17.463655	-0.157847	3.081020
839.489408	3154.913855	17.468659	-0.157853	3.077322
839.564906	3146.861353	17.473664	-0.157862	3.073615
839.460364	3138.855099	17.478669	-0.157837	3.069917
839.453413	3130.841175	17.483674	-0.157830	3.066215
840.014038	3122.777649	17.488679	-0.157930	3.062512
839.731020	3114.865129	17.493683	-0.157872	3.058835
839.024103	3107.000323	17.498688	-0.157735	3.055155
839.226122	3098.952552	17.503693	-0.157767	3.051429
838.864541	3090.971138	17.508698	-0.157694	3.047703
839.073401	3082.944912	17.513703	-0.157728	3.043979
839.304481	3074.932807	17.518707	-0.157766	3.040257
839.270279	3066.979912	17.523712	-0.157754	3.036546
839.207963	3059.020297	17.528717	-0.157737	3.032826
839.260019	3050.973863	17.533722	-0.157742	3.029066
839.420615	3042.994748	17.538727	-0.157766	3.025338
839.428334	3035.010700	17.543731	-0.157762	3.021596
839.026743	3027.067976	17.548736	-0.157682	3.017849
839.035065	3019.106392	17.553741	-0.157679	3.014108
838.920018	3011.092682	17.558746	-0.157652	3.010332
839.068382	3003.075341	17.563751	-0.157674	3.006563
839.129822	2995.102259	17.568755	-0.157680	3.002805
839.138847	2987.119546	17.573760	-0.157677	2.999035
838.872113	2979.239984	17.578765	-0.157622	2.995296
838.957210	2971.169756	17.583770	-0.157632	2.991480
838.822536	2963.224557	17.588775	-0.157602	2.987706
838.952949	2955.171272	17.593779	-0.157621	2.983890
839.628306	2947.082738	17.598784	-0.157741	2.980080
839.454325	2939.185172	17.603789	-0.157704	2.976313
838.708706	2931.314840	17.608794	-0.157560	2.972525
838.962102	2923.259163	17.613799	-0.157601	2.968695
838.609552	2915.347244	17.618803	-0.157531	2.964897
838.289135	2907.431111	17.623808	-0.157466	2.961094
838.088048	2899.448647	17.628813	-0.157423	2.957261
838.215284	2891.374916	17.633818	-0.157441	2.953395
838.521474	2883.355402	17.638823	-0.157493	2.949560
838.217031	2875.396596	17.643827	-0.157431	2.945718
838.453960	2867.374803	17.648832	-0.157470	2.941868
838.910461	2859.344741	17.653837	-0.157549	2.938021
838.703561	2851.376377	17.658842	-0.157506	2.934164
838.318227	2843.474822	17.663847	-0.157429	2.930324
838.172710	2835.513836	17.668851	-0.157396	2.926464
838.155753	2827.513977	17.673856	-0.157388	2.922586
838.123498	2819.588785	17.678861	-0.157377	2.918738
837.966704	2811.586270	17.683866	-0.157342	2.914841
837.632928	2803.594746	17.688871	-0.157275	2.910935
837.161595	2795.667689	17.693875	-0.157182	2.907047
837.008710	2787.640924	17.698880	-0.157148	2.903123
837.084271	2779.630519	17.703885	-0.157157	2.899214
837.046661	2771.633196	17.708890	-0.157144	2.895299
836.963534	2763.646658	17.713895	-0.157124	2.891382
836.961256	2755.659468	17.718899	-0.157118	2.887464
837.150523	2747.632601	17.723904	-0.157148	2.883532
837.184350	2739.704306	17.728909	-0.157149	2.879634
836.984788	2731.720294	17.733914	-0.157106	2.875691
836.872029	2723.786345	17.738919	-0.157080	2.871771
836.947699	2715.774595	17.743923	-0.157089	2.867819
836.869962	2707.760150	17.748928	-0.157069	2.863850
836.759664	2699.826659	17.753933	-0.157043	2.859915
836.865940	2691.797987	17.758938	-0.157058	2.855939
836.719280	2683.864242	17.763943	-0.157025	2.851991
837.277108	2675.761612	17.768947	-0.157124	2.847993
836.820959	2667.867484	17.773952	-0.157033	2.844035
836.909806	2659.938456	17.778957	-0.157045	2.840086
836.606145	2651.980641	17.783962	-0.156983	2.836095
836.608091	2643.984465	17.788967	-0.156978	2.832096
836.735987	2635.976510	17.793971	-0.156997	2.828092
837.257674	2627.840331	17.798976	-0.157088	2.824042
837.078137	2619.988262	17.803981	-0.157050	2.820087
836.643703	2612.072904	17.808986	-0.156964	2.816081
836.597867	2604.090406	17.813991	-0.156950	2.812058
836.489267	2596.106158	17.818995	-0.156924	2.808024
836.285068	2588.129624	17.824000	-0.156881	2.803983
836.322586	2580.194804	17.829005	-0.156883	2.799971
835.896017	2572.232557	17.834010	-0.156798	2.795913
836.319363	2564.169030	17.839015	-0.156871	2.791847
836.397891	2556.179076	17.844019	-0.156881	2.787792
836.879283	2548.088336	17.849024	-0.156965	2.783704
835.999103	2540.324859	17.854029	-0.156796	2.779696
836.164208	2532.269763	17.859034	-0.156821	2.775595
836.291413	2524.279736	17.864039	-0.156840	2.771519
836.016413	2516.336804	17.869043	-0.156783	2.767437
835.769336	2508.395171	17.874048	-0.156732	2.763352
836.041012	2500.386373	17.879053	-0.156777	2.759257
835.929668	2492.407587	17.884058	-0.156751	2.755149
835.806059	2484.399792	17.889063	-0.156723	2.751018
835.973095	2476.377109	17.894067	-0.156749	2.746892
835.867113	2468.408270	17.899072	-0.156724	2.742770
835.441616	2460.544128	17.904077	-0.156639	2.738677
835.684056	2452.474976	17.909082	-0.156679	2.734512
835.861299	2444.485244	17.914087	-0.156707	2.730378
835.489087	2436.561969	17.919091	-0.156632	2.726239
835.488005	2428.577404	17.924096	-0.156627	2.722084
835.536207	2420.614120	17.929101	-0.156630	2.717937
835.445100	2412.631773	17.934106	-0.156608	2.713765
835.102058	2404.712761	17.939111	-0.156539	2.709604
835.167684	2396.696389	17.944115	-0.156546	2.705411
835.263232	2388.709043	17.949120	-0.156558	2.701229
835.220637	2380.773774	17.954125	-0.156545	2.697059
835.175497	2372.757398	17.959130	-0.156532	2.692839
835.722727	2364.703527	17.964135	-0.156628	2.688631
835.693008	2356.742243	17.969139	-0.156617	2.684429
835.958067	2348.752485	17.974144	-0.156661	2.680223
836.111648	2340.801579	17.979149	-0.156685	2.676025
835.751479	2332.880657	17.984154	-0.156612	2.671803
835.704581	2324.887398	17.989159	-0.156598	2.667555
835.951751	2316.903957	17.994163	-0.156639	2.663326
835.437007	2309.014206	17.999168	-0.156538	2.659090
835.479615	2301.032445	18.004173	-0.156541	2.654834
835.139907	2293.088894	18.009178	-0.156472	2.650567
835.281620	2285.085675	18.014183	-0.156493	2.646293
835.182925	2277.130608	18.019187	-0.156470	2.642022
835.211186	2269.145849	18.024192	-0.156470	2.637736
834.724701	2261.266388	18.029197	-0.156374	2.633466
834.926223	2253.196201	18.034202	-0.156406	2.629132
834.966192	2245.204810	18.039207	-0.156408	2.624822
834.714788	2237.286781	18.044211	-0.156356	2.620525
834.582278	2229.337198	18.049216	-0.156326	2.616213
834.682433	2221.321034	18.054221	-0.156339	2.611872
834.334579	2213.369763	18.059226	-0.156269	2.607530
834.910198	2205.303862	18.064231	-0.156371	2.603180
834.335153	2197.471745	18.069235	-0.156259	2.598873
834.222001	2189.485597	18.074240	-0.156233	2.594505
834.429963	2181.371856	18.079245	-0.156266	2.590082
834.409494	2173.372478	18.084250	-0.156257	2.585699
833.722202	2165.559535	18.089255	-0.156124	2.581365
833.696506	2157.571477	18.094259	-0.156114	2.576972
834.199727	2149.486618	18.099264	-0.156202	2.572556
833.897013	2141.587554	18.104269	-0.156140	2.568178
833.757981	2133.630105	18.109274	-0.156109	2.563772
833.911066	2125.641049	18.114279	-0.156132	2.559362
833.688608	2117.731479	18.119283	-0.156086	2.554961
833.651316	2109.733278	18.124288	-0.156073	2.550517
833.948476	2101.718918	18.129293	-0.156123	2.546079
833.619427	2093.799073	18.134298	-0.156057	2.541643
833.374894	2085.864052	18.139303	-0.156006	2.537195
833.400146	2077.885818	18.144307	-0.156006	2.532736
833.484328	2069.882352	18.149312	-0.156016	2.528258
832.943594	2062.007954	18.154317	-0.155910	2.523800
833.121590	2053.997749	18.159322	-0.155938	2.519309
833.684492	2045.942361	18.164327	-0.156037	2.514813
832.821982	2038.130334	18.169331	-0.155872	2.510343
833.432967	2030.004903	18.174336	-0.155980	2.505794
833.406917	2022.058286	18.179341	-0.155970	2.501292
833.457818	2014.087187	18.184346	-0.155974	2.496774
832.725445	2006.249838	18.189351	-0.155832	2.492266
832.502775	1998.296214	18.194355	-0.155786	2.487721
833.149941	1990.193080	18.199360	-0.155901	2.483147
833.185549	1982.264929	18.204365	-0.155902	2.478619
832.966931	1974.306110	18.209370	-0.155856	2.474047
832.614712	1966.419234	18.214375	-0.155785	2.469497
832.334320	1958.489971	18.219379	-0.155728	2.464920
832.378955	1950.482765	18.224384	-0.155731	2.460313
832.578091	1942.495455	18.229389	-0.155763	2.455721
832.352721	1934.534843	18.234394	-0.155716	2.451104
832.209104	1926.599920	18.239399	-0.155684	2.446499
832.055686	1918.650658	18.244403	-0.155650	2.441877
832.311783	1910.631790	18.249408	-0.155692	2.437236
832.038171	1902.726489	18.254413	-0.155636	2.432612
832.026155	1894.677285	18.259418	-0.155628	2.427916
832.010155	1886.733564	18.264423	-0.155620	2.423272
832.245341	1878.745995	18.269427	-0.155659	2.418612
831.582119	1870.867234	18.274432	-0.155530	2.413938
831.562962	1862.897431	18.279437	-0.155521	2.409251
831.528413	1854.908651	18.284442	-0.155509	2.404542
831.887230	1846.913283	18.289447	-0.155571	2.399852
832.083832	1838.931464	18.294451	-0.155602	2.395147
831.787049	1831.014489	18.299456	-0.155542	2.390433
832.085018	1823.023279	18.304461	-0.155592	2.385712
831.283418	1815.204105	18.309466	-0.155437	2.380997
831.131446	1807.261226	18.314471	-0.155404	2.376250
830.983910	1799.293240	18.319475	-0.155371	2.371480
830.588525	1791.358815	18.324480	-0.155292	2.366699
830.866561	1783.359331	18.329485	-0.155339	2.361925
830.738145	1775.407556	18.334490	-0.155309	2.357136
830.883055	1767.404015	18.339495	-0.155331	2.352329
830.968855	1759.402238	18.344499	-0.155342	2.347508
831.011198	1751.421171	18.349504	-0.155344	2.342686
830.587305	1743.562987	18.354509	-0.155260	2.337891
830.230863	1735.625214	18.359514	-0.155189	2.333043
830.227180	1727.650283	18.364519	-0.155183	2.328191
830.607017	1719.607487	18.369523	-0.155248	2.323319
830.532191	1711.689270	18.374528	-0.155229	2.318476
830.505473	1703.753557	18.379533	-0.155219	2.313615
831.013639	1695.692967	18.384538	-0.155308	2.308713
830.690459	1687.802869	18.389543	-0.155242	2.303835
830.728712	1679.867696	18.394547	-0.155244	2.298950
830.428961	1671.960433	18.399552	-0.155183	2.294042
830.588835	1663.992929	18.404557	-0.155208	2.289126
830.021191	1656.112230	18.409562	-0.155097	2.284191
830.077983	1648.149983	18.414567	-0.155102	2.279248
830.158073	1640.192722	18.419571	-0.155112	2.274300
830.217449	1632.150646	18.424576	-0.155118	2.269286
829.869931	1624.252967	18.429581	-0.155048	2.264316
829.848956	1616.278296	18.434586	-0.155038	2.259315
829.881356	1608.323795	18.439591	-0.155039	2.254320
829.897776	1600.368803	18.444595	-0.155037	2.249312
829.583197	1592.446736	18.449600	-0.154973	2.244285
829.540873	1584.538658	18.454605	-0.154960	2.239280
829.358072	1576.601247	18.459610	-0.154921	2.234232
829.044443	1568.677123	18.464615	-0.154857	2.229170
829.460933	1560.626306	18.469619	-0.154929	2.224080
829.141889	1552.722212	18.474624	-0.154865	2.219007
829.029244	1544.815450	18.479629	-0.154838	2.213938
829.096737	1536.819567	18.484634	-0.154846	2.208817
828.961520	1528.879939	18.489639	-0.154815	2.203703
828.384889	1521.052080	18.494643	-0.154703	2.198608
828.237755	1513.089119	18.499648	-0.154670	2.193453
828.595717	1505.068455	18.504653	-0.154731	2.188294
828.306588	1497.135502	18.509658	-0.154672	2.183121
828.234970	1489.198842	18.514663	-0.154654	2.177953
828.362198	1481.217170	18.519667	-0.154672	2.172763
828.005588	1473.312305	18.524672	-0.154600	2.167564
828.343811	1465.287450	18.529677	-0.154658	2.162340
828.478388	1457.331905	18.534682	-0.154678	2.157129
829.057459	1449.282710	18.539687	-0.154780	2.151886
828.908187	1441.406714	18.544691	-0.154747	2.146676
828.127363	1433.624574	18.549696	-0.154597	2.141455
828.082226	1425.696975	18.554701	-0.154583	2.136195
827.650265	1417.808570	18.559706	-0.154497	2.130911
827.452296	1409.848357	18.564711	-0.154455	2.125589
827.442831	1401.923786	18.569715	-0.154448	2.120294
827.164719	1394.001848	18.574720	-0.154391	2.114963
827.262256	1385.999862	18.579725	-0.154404	2.109600
826.987152	1378.056941	18.584730	-0.154348	2.104228
826.829973	1370.164557	18.589735	-0.154313	2.098887
826.646566	1362.220571	18.594739	-0.154274	2.093495
826.628923	1354.222312	18.599744	-0.154265	2.088068
826.829584	1346.263090	18.604749	-0.154297	2.082676
826.541750	1338.379388	18.609754	-0.154238	2.077272
826.354136	1330.454811	18.614759	-0.154198	2.071837
826.154522	1322.545397	18.619763	-0.154156	2.066396
825.946557	1314.612112	18.624768	-0.154112	2.060924
825.728079	1306.733025	18.629773	-0.154066	2.055473
825.149338	1298.834337	18.634778	-0.153953	2.049958
825.118386	1290.866180	18.639783	-0.153942	2.044435
825.130110	1282.950543	18.644787	-0.153939	2.038938
824.347758	1275.096008	18.649792	-0.153788	2.033387
824.493656	1267.094670	18.654797	-0.153810	2.027814
824.208995	1259.157310	18.659802	-0.153752	2.022226
823.279387	1251.353967	18.664807	-0.153573	2.016650
823.016349	1243.406636	18.669811	-0.153519	2.011026
822.809363	1235.433030	18.674816	-0.153475	2.005373
821.569870	1227.692549	18.679821	-0.153239	1.999761
821.527687	1219.669748	18.684826	-0.153226	1.994059
820.512708	1211.856068	18.689831	-0.153032	1.988386
819.621841	1203.972165	18.694835	-0.152861	1.982659
818.290342	1196.156080	18.699840	-0.152608	1.976918
817.185291	1188.283340	18.704845	-0.152397	1.971142
815.507557	1180.481842	18.709850	-0.152079	1.965340
813.846265	1172.653344	18.714855	-0.151765	1.959501
811.236064	1164.960957	18.719859	-0.151274	1.953641
808.585471	1157.177299	18.724864	-0.150775	1.947691
806.377126	1149.297903	18.729869	-0.150358	1.941700
803.459270	1141.540771	18.734874	-0.149810	1.935702
801.208178	1133.658802	18.739879	-0.149386	1.929667
799.532318	1125.681112	18.744883	-0.149068	1.923605
797.953286	1117.703777	18.749888	-0.148769	1.917534
796.604541	1109.725376	18.754893	-0.148513	1.911469
795.164700	1101.770473	18.759898	-0.148239	1.905392
793.275402	1093.920149	18.764903	-0.147882	1.899321
791.970207	1085.969138	18.769907	-0.147634	1.893222
790.947381	1077.942376	18.774912	-0.147438	1.887078
789.482871	1070.074611	18.779917	-0.147160	1.880983
788.338559	1062.116558	18.784922	-0.146942	1.874836
786.582838	1054.305820	18.789927	-0.146610	1.868709
785.391009	1046.360888	18.794931	-0.146383	1.862526
784.578615	1038.346940	18.799936	-0.146226	1.856313
783.809435	1030.367121	18.804941	-0.146077	1.850110
782.773736	1022.440400	18.809946	-0.145879	1.843895
782.191446	1014.477920	18.814951	-0.145766	1.837685
780.968512	1006.632313	18.819955	-0.145533	1.831468
779.428076	998.795282	18.824960	-0.145241	1.825199
778.454416	990.898160	18.829965	-0.145054	1.818928
777.637291	982.948558	18.834970	-0.144897	1.812613
776.681062	975.026636	18.839975	-0.144714	1.806281
775.663857	967.160389	18.844979	-0.144519	1.799963
774.313276	959.332137	18.849984	-0.144262	1.793611
773.485455	951.369589	18.854989	-0.144103	1.787194
772.072248	943.544951	18.859994	-0.143834	1.780791
770.612479	935.729880	18.864999	-0.143557	1.774367
769.366068	927.855255	18.870003	-0.143320	1.767897
768.066178	919.975383	18.875008	-0.143073	1.761392
767.092404	912.080878	18.880013	-0.142886	1.754892
765.762218	904.219204	18.885018	-0.142633	1.748349
764.965414	896.257415	18.890023	-0.142480	1.741768
763.593191	888.459558	18.895027	-0.142219	1.735222
762.634462	880.533101	18.900032	-0.142035	1.728598
761.323004	872.724957	18.905037	-0.141786	1.722000
760.642476	864.760865	18.910042	-0.141654	1.715329
759.361061	856.932053	18.915047	-0.141410	1.708666
758.267593	849.058231	18.920051	-0.141201	1.701964
756.547285	841.294419	18.925056	-0.140876	1.695243
755.709650	833.366546	18.930061	-0.140715	1.688475
754.632671	825.482172	18.935066	-0.140509	1.681685
753.364054	817.664750	18.940071	-0.140268	1.674897
752.620869	809.742801	18.945075	-0.140124	1.668063
751.387039	801.896220	18.950080	-0.139889	1.661199
750.230458	794.075186	18.955085	-0.139668	1.654338
749.196354	786.186965	18.960090	-0.139471	1.647407
748.517269	778.274539	18.965095	-0.139339	1.640475
747.319544	770.472036	18.970099	-0.139111	1.633536
746.144956	762.601201	18.975104	-0.138887	1.626511
745.577684	754.689157	18.980109	-0.138776	1.619505
744.434022	746.859819	18.985114	-0.138558	1.612459
742.720019	739.136061	18.990119	-0.138234	1.605394
742.297567	731.195465	18.995123	-0.138150	1.598289
741.238196	723.355273	19.000128	-0.137947	1.591150
740.019947	715.563208	19.005133	-0.137715	1.583999
738.651835	707.788822	19.010138	-0.137455	1.576810
738.156383	699.851499	19.015143	-0.137358	1.569567
737.220887	692.023795	19.020147	-0.137178	1.562325
735.878284	684.251601	19.025152	-0.136923	1.555040
735.230520	676.372566	19.030157	-0.136797	1.547725
734.089024	668.568059	19.035162	-0.136580	1.540370
732.786659	660.811527	19.040167	-0.136332	1.532999
732.460640	652.849176	19.045171	-0.136266	1.525549
731.523526	645.049680	19.050176	-0.136086	1.518121
730.896692	637.178904	19.055181	-0.135965	1.510637
729.992198	629.370980	19.060186	-0.135791	1.503132
729.210805	621.556976	19.065191	-0.135640	1.495603
728.299303	613.760006	19.070195	-0.135465	1.488030
727.184710	605.993754	19.075200	-0.135253	1.480417
726.359011	598.203395	19.080205	-0.135094	1.472786
725.550045	590.347819	19.085210	-0.134938	1.465054
724.888413	582.523998	19.090215	-0.134810	1.457336
723.930810	574.754920	19.095219	-0.134626	1.449582
722.954791	566.977878	19.100224	-0.134439	1.441775
721.886900	559.251526	19.105229	-0.134235	1.433961
721.054044	551.440175	19.110234	-0.134075	1.426057
719.983344	543.708208	19.115239	-0.133870	1.418149
719.087945	535.936512	19.120243	-0.133699	1.410186
717.823174	528.217566	19.125248	-0.133458	1.402168
716.911251	520.466347	19.130253	-0.133283	1.394131
715.932970	512.691756	19.135258	-0.133096	1.386011
715.373980	504.853808	19.140263	-0.132986	1.377850
714.529426	497.091071	19.145267	-0.132824	1.369668
713.490468	489.361962	19.150272	-0.132625	1.361439
712.659005	481.616853	19.155277	-0.132466	1.353178
711.593714	473.896382	19.160282	-0.132262	1.344851
711.079909	466.097787	19.165287	-0.132161	1.336487
710.217555	458.360891	19.170291	-0.131995	1.328073
709.492248	450.600370	19.175296	-0.131855	1.319605
708.727626	442.830172	19.180301	-0.131708	1.311064
707.900984	435.054874	19.185306	-0.131549	1.302449
706.953406	427.370450	19.190311	-0.131367	1.293855
706.318877	419.632436	19.195315	-0.131244	1.285201
705.111646	412.015920	19.200320	-0.131014	1.276517
704.141291	404.342378	19.205325	-0.130828	1.267753
703.273664	396.644714	19.210330	-0.130662	1.258921
702.859820	388.879657	19.215335	-0.130579	1.250036
701.587670	381.293006	19.220339	-0.130338	1.241125
700.502281	373.655690	19.225344	-0.130130	1.232127
700.093887	365.890406	19.230349	-0.130049	1.223048
699.189802	358.249814	19.235354	-0.129876	1.213948
697.963721	350.644699	19.240359	-0.129642	1.204755
697.371776	342.955645	19.245363	-0.129527	1.195521
696.605544	335.286004	19.250368	-0.129379	1.186201
695.377986	327.743725	19.255373	-0.129146	1.176867
694.806840	320.040402	19.260378	-0.129034	1.167397
693.700950	312.482017	19.265383	-0.128823	1.157916
692.634805	304.900811	19.270387	-0.128620	1.148335
691.338644	297.347750	19.275392	-0.128373	1.138660
690.772969	289.683221	19.280397	-0.128263	1.128919
689.509486	282.165101	19.285402	-0.128023	1.119126
688.638899	274.579745	19.290407	-0.127856	1.109246
688.245530	266.907764	19.295411	-0.127777	1.099272
686.946963	259.413733	19.300416	-0.127531	1.089235
686.189381	251.847389	19.305421	-0.127384	1.079131
685.140488	244.337261	19.310426	-0.127184	1.068939
684.050279	236.834623	19.315431	-0.126976	1.058650
682.856953	229.377275	19.320435	-0.126749	1.048295
681.609764	221.919327	19.325440	-0.126512	1.037824
680.249212	214.500031	19.330445	-0.126254	1.027271
679.636645	206.939155	19.335450	-0.126135	1.016592
679.137907	199.386838	19.340455	-0.126037	1.005839
677.434452	192.092509	19.345459	-0.125715	0.995038
675.667012	184.755824	19.350464	-0.125381	0.984041
674.899046	177.267374	19.355469	-0.125233	0.972952
673.563408	169.900387	19.360474	-0.124979	0.961767
672.205746	162.553604	19.365479	-0.124721	0.950475
670.555641	155.271255	19.370483	-0.124409	0.939066
667.001036	148.314618	19.375488	-0.123743	0.927503
658.490340	142.194808	19.380493	-0.122154	0.915743
642.959421	137.111655	19.385498	-0.119259	0.903516
622.737501	132.606466	19.390503	-0.115491	0.890718
605.283573	127.403243	19.395507	-0.112237	0.877377
593.704663	121.035616	19.400512	-0.110077	0.863604
582.708273	114.555331	19.405517	-0.108025	0.849584
567.167809	108.830895	19.410522	-0.105128	0.835241
551.970841	102.931619	19.415527	-0.102294	0.820438
543.865832	95.799626	19.420531	-0.100780	0.805391
540.535816	87.939688	19.425536	-0.100155	0.790265
535.629593	80.696718	19.430541	-0.099237	0.775464