Mon Apr 19 09:24:02 2021

Number of Points = 3631
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.559741	0.107685	0.000000	0.000111	0.308937

2.810762	0.062673	0.005005	0.000064	0.308939
3.567926	-0.080879	0.010010	-0.000077	0.308911
3.207266	-0.009164	0.015014	-0.000010	0.308940
3.446157	-0.054477	0.020019	-0.000054	0.308931
4.117654	-0.179636	0.025024	-0.000179	0.308916
3.579430	-0.106722	0.030029	-0.000079	0.308799
3.475598	-0.126696	0.035034	-0.000059	0.308617
3.487113	-0.126516	0.040038	-0.000062	0.308627
3.341364	-0.101608	0.045043	-0.000034	0.308619
3.025009	-0.043988	0.050048	0.000025	0.308620
3.044154	-0.045860	0.055053	0.000021	0.308627
2.977522	-0.035290	0.060058	0.000033	0.308620
2.841806	-0.008293	0.065062	0.000059	0.308630
3.222800	-0.082141	0.070067	-0.000012	0.308609
3.238357	-0.084189	0.075072	-0.000015	0.308612
3.274197	-0.106736	0.080077	-0.000022	0.308537
3.346868	-0.174755	0.085082	-0.000035	0.308279
3.201121	-0.144756	0.090086	-0.000008	0.308296
2.708444	-0.053449	0.095091	0.000084	0.308304
3.052543	-0.117545	0.100096	0.000020	0.308296
3.647423	-0.226217	0.105101	-0.000091	0.308293
3.722224	-0.255436	0.110106	-0.000105	0.308220
3.601790	-0.279199	0.115110	-0.000082	0.308005
3.744166	-0.309085	0.120115	-0.000109	0.307986
3.646777	-0.289384	0.125120	-0.000090	0.307995
3.414346	-0.244216	0.130125	-0.000047	0.308009
2.894727	-0.219157	0.135130	0.000050	0.307683
2.845122	-0.211991	0.140134	0.000059	0.307674
3.051754	-0.250548	0.145139	0.000021	0.307669
2.608018	-0.167466	0.150144	0.000103	0.307680
2.653244	-0.195498	0.155149	0.000095	0.307587
2.788606	-0.268894	0.160154	0.000070	0.307357
3.123042	-0.328608	0.165158	0.000008	0.307362
2.350603	-0.184079	0.170163	0.000151	0.307381
2.849693	-0.297550	0.175168	0.000058	0.307273
2.950519	-0.363180	0.180173	0.000040	0.307050
2.742340	-0.327235	0.185178	0.000079	0.307041
3.155342	-0.401387	0.190182	0.000002	0.307045
2.716536	-0.373710	0.195187	0.000084	0.306800
2.078603	-0.263899	0.200192	0.000202	0.306771
1.924618	-0.234319	0.205197	0.000231	0.306778
1.988422	-0.257611	0.210202	0.000219	0.306723
1.971790	-0.314572	0.215206	0.000222	0.306439
1.884780	-0.299650	0.220211	0.000239	0.306435
2.802062	-0.469807	0.225216	0.000068	0.306418
2.998619	-0.558564	0.230221	0.000031	0.306168
2.854973	-0.544886	0.235226	0.000058	0.306109
2.869676	-0.555594	0.240230	0.000056	0.306070
3.399092	-0.714428	0.245235	-0.000043	0.305774
3.459891	-0.726886	0.250240	-0.000054	0.305767
3.011231	-0.683453	0.255245	0.000029	0.305587
2.629427	-0.624324	0.260250	0.000100	0.305538
2.272183	-0.576409	0.265254	0.000167	0.305457
1.595993	-0.505467	0.270259	0.000293	0.305211
2.420374	-0.659887	0.275264	0.000140	0.305189
2.335823	-0.681451	0.280269	0.000155	0.305013
2.529418	-0.749133	0.285274	0.000119	0.304859
2.608523	-0.776789	0.290278	0.000105	0.304796
3.180479	-0.935719	0.295283	-0.000002	0.304534
2.853150	-0.882711	0.300288	0.000059	0.304503
3.506978	-1.053566	0.305293	-0.000062	0.304256
3.355433	-1.043620	0.310298	-0.000034	0.304172
3.203560	-1.069270	0.315302	-0.000006	0.303918
2.083575	-0.877980	0.320307	0.000203	0.303860
2.198255	-0.951683	0.325312	0.000182	0.303608
2.393331	-0.993633	0.330317	0.000145	0.303576
2.099892	-1.003133	0.335322	0.000200	0.303277
1.277096	-0.849815	0.340326	0.000353	0.303295
2.029492	-1.047919	0.345331	0.000213	0.303001
2.350704	-1.107642	0.350336	0.000154	0.302995
2.503541	-1.205393	0.355341	0.000125	0.302660
2.688955	-1.250538	0.360346	0.000091	0.302605
3.089456	-1.377705	0.365350	0.000016	0.302345
3.066589	-1.408577	0.370355	0.000021	0.302177
3.412778	-1.508508	0.375360	-0.000044	0.301999
3.762227	-1.623076	0.380365	-0.000109	0.301754
3.542995	-1.617955	0.385370	-0.000068	0.301588
2.778605	-1.519702	0.390374	0.000075	0.301392
1.596535	-1.350647	0.395379	0.000295	0.301172
1.300475	-1.311480	0.400384	0.000350	0.301102
0.863545	-1.292239	0.405389	0.000431	0.300812
0.331320	-1.205876	0.410394	0.000530	0.300762
0.573292	-1.292859	0.415398	0.000485	0.300555
1.249732	-1.425127	0.420403	0.000359	0.300510
1.353358	-1.508838	0.425408	0.000340	0.300197
2.425009	-1.729618	0.430413	0.000141	0.300072
2.437862	-1.771425	0.435418	0.000139	0.299881
2.435356	-1.829714	0.440422	0.000139	0.299597
2.397248	-1.854980	0.445427	0.000146	0.299441
2.782153	-1.962827	0.450432	0.000075	0.299258
2.599238	-1.996814	0.455437	0.000109	0.298933
2.107398	-1.949926	0.460442	0.000200	0.298727
1.041510	-1.780668	0.465446	0.000399	0.298608
0.664371	-1.776335	0.470451	0.000469	0.298296
-0.095905	-1.659845	0.475456	0.000611	0.298191
0.100641	-1.732532	0.480461	0.000574	0.298011
0.244770	-1.808417	0.485466	0.000547	0.297770
0.343392	-1.848991	0.490470	0.000529	0.297659
0.970752	-2.024815	0.495475	0.000412	0.297359
1.455101	-2.146547	0.500480	0.000322	0.297194
2.014888	-2.290434	0.505485	0.000218	0.296989
1.310007	-2.209138	0.510490	0.000350	0.296760
0.892559	-2.189058	0.515494	0.000427	0.296488
0.176362	-2.089744	0.520499	0.000561	0.296337
0.564426	-2.205698	0.525504	0.000488	0.296115
0.549448	-2.257895	0.530509	0.000491	0.295846
-0.016997	-2.187377	0.535514	0.000597	0.295688
-1.247332	-1.987908	0.540518	0.000826	0.295569
-1.474568	-2.005053	0.545523	0.000868	0.295283
-0.717808	-2.167898	0.550528	0.000727	0.295158
-0.304027	-2.294400	0.555533	0.000651	0.294907
-0.758473	-2.261161	0.560538	0.000735	0.294664
-0.354270	-2.371801	0.565542	0.000660	0.294481
-0.606299	-2.371294	0.570547	0.000707	0.294258
-0.680268	-2.410900	0.575552	0.000721	0.293997
-1.148212	-2.359257	0.580557	0.000808	0.293832
-2.010955	-2.241453	0.585562	0.000969	0.293640
-1.690918	-2.350937	0.590566	0.000909	0.293387
-2.221442	-2.282877	0.595571	0.001008	0.293247
-2.674893	-2.247836	0.600576	0.001092	0.293012
-2.638141	-2.289439	0.605581	0.001086	0.292840
-2.661845	-2.318801	0.610586	0.001090	0.292673
-2.629106	-2.385254	0.615590	0.001084	0.292374
-3.193400	-2.304023	0.620595	0.001189	0.292268
-3.688270	-2.257924	0.625600	0.001281	0.292050
-3.952379	-2.245227	0.630605	0.001331	0.291875
-3.910949	-2.277812	0.635610	0.001323	0.291750
-3.640900	-2.386938	0.640614	0.001273	0.291452
-4.109735	-2.322132	0.645619	0.001360	0.291351
-4.825186	-2.239286	0.650624	0.001493	0.291116
-4.627296	-2.299195	0.655629	0.001456	0.290997
-5.099676	-2.250802	0.660634	0.001544	0.290810
-4.963642	-2.308491	0.665638	0.001519	0.290646
-5.465236	-2.236672	0.670643	0.001613	0.290549
-5.538543	-2.278242	0.675648	0.001626	0.290275
-5.859181	-2.230285	0.680653	0.001686	0.290224
-6.323732	-2.205174	0.685658	0.001773	0.289927
-6.401344	-2.193709	0.690662	0.001787	0.289914
-6.864728	-2.172588	0.695667	0.001873	0.289598
-6.994841	-2.153782	0.700672	0.001898	0.289574
-6.558821	-2.284801	0.705677	0.001817	0.289315
-7.022265	-2.207318	0.710682	0.001903	0.289281
-7.026544	-2.269949	0.715686	0.001904	0.288963
-7.259692	-2.231349	0.720691	0.001947	0.288944
-7.541036	-2.238615	0.725696	0.002000	0.288651
-7.514935	-2.246070	0.730701	0.001995	0.288637
-7.638590	-2.287246	0.735706	0.002018	0.288318
-7.910136	-2.238271	0.740710	0.002068	0.288316
-7.719655	-2.329548	0.745715	0.002033	0.288031
-7.923601	-2.297882	0.750720	0.002071	0.288003
-8.334325	-2.284325	0.755725	0.002148	0.287696
-8.464009	-2.266529	0.760730	0.002172	0.287667
-8.813659	-2.256814	0.765734	0.002237	0.287395
-8.742666	-2.279605	0.770739	0.002224	0.287345
-8.822216	-2.318871	0.775744	0.002239	0.287074
-9.173498	-2.261930	0.780749	0.002304	0.287039
-9.742080	-2.202086	0.785754	0.002410	0.286819
-9.582144	-2.245268	0.790758	0.002380	0.286748
-10.004582	-2.202862	0.795763	0.002459	0.286574
-10.279024	-2.185471	0.800768	0.002510	0.286410
-9.884375	-2.274188	0.805773	0.002437	0.286324
-10.368575	-2.229924	0.810778	0.002527	0.286102
-10.677316	-2.175276	0.815782	0.002584	0.286094
-11.510702	-2.078576	0.820787	0.002740	0.285817
-11.332042	-2.111944	0.825792	0.002706	0.285812
-11.462850	-2.115610	0.830797	0.002731	0.285673
-11.732387	-2.090350	0.835802	0.002781	0.285552
-10.575668	-2.319328	0.840806	0.002566	0.285457
-11.127636	-2.271791	0.845811	0.002669	0.285189
-11.880631	-2.132208	0.850816	0.002809	0.285203
-11.698041	-2.223959	0.855821	0.002775	0.284905
-11.667214	-2.238086	0.860826	0.002769	0.284862
-11.412928	-2.327187	0.865830	0.002722	0.284643
-12.356310	-2.173466	0.870835	0.002898	0.284553
-12.041117	-2.255835	0.875840	0.002839	0.284425
-12.264436	-2.246705	0.880845	0.002881	0.284264
-12.747595	-2.163241	0.885850	0.002971	0.284242
-12.167668	-2.333393	0.890854	0.002863	0.283912
-12.798941	-2.215707	0.895859	0.002980	0.283927
-13.292008	-2.171969	0.900864	0.003072	0.283692
-13.891895	-2.071406	0.905869	0.003184	0.283649
-13.778208	-2.104452	0.910874	0.003163	0.283585
-13.757152	-2.162173	0.915878	0.003159	0.283310
-13.797728	-2.155800	0.920883	0.003166	0.283304
-13.708137	-2.211279	0.925888	0.003150	0.283104
-13.797667	-2.213615	0.930893	0.003166	0.283008
-13.937980	-2.209392	0.935898	0.003193	0.282899
-14.280157	-2.191931	0.940902	0.003256	0.282670
-14.445674	-2.161171	0.945907	0.003287	0.282673
-14.978976	-2.111520	0.950912	0.003387	0.282431
-15.334997	-2.057215	0.955917	0.003453	0.282377
-15.531009	-2.020651	0.960922	0.003489	0.282381
-15.264225	-2.130778	0.965926	0.003440	0.282065
-15.776894	-2.038575	0.970931	0.003535	0.282060
-15.684320	-2.072639	0.975936	0.003518	0.281971
-15.539562	-2.139475	0.980941	0.003491	0.281763
-15.815178	-2.091583	0.985946	0.003543	0.281751
-15.727319	-2.150106	0.990950	0.003526	0.281532
-16.058065	-2.110920	0.995955	0.003588	0.281424
-15.912625	-2.144170	1.000960	0.003561	0.281389
-16.572588	-2.074422	1.005965	0.003684	0.281130
-16.590942	-2.073491	1.010970	0.003687	0.281117
-16.513861	-2.108525	1.015974	0.003673	0.281009
-16.857402	-2.086924	1.020979	0.003737	0.280798
-16.737743	-2.110350	1.025984	0.003715	0.280789
-16.954813	-2.096037	1.030989	0.003755	0.280659
-17.716173	-1.972790	1.035994	0.003897	0.280581
-17.730156	-1.968977	1.040998	0.003900	0.280587
-17.489974	-2.068615	1.046003	0.003855	0.280298
-17.709909	-2.040067	1.051008	0.003896	0.280239
-17.951572	-1.995774	1.056013	0.003941	0.280240
-18.079735	-2.034595	1.061018	0.003965	0.279919
-17.646590	-2.113430	1.066022	0.003884	0.279918
-18.228507	-2.025153	1.071027	0.003993	0.279827
-18.222366	-2.074644	1.076032	0.003992	0.279577
-17.837006	-2.142375	1.081037	0.003920	0.279589
-18.572660	-2.045399	1.086042	0.004057	0.279398
-18.817523	-2.020593	1.091046	0.004103	0.279295
-18.655640	-2.049348	1.096051	0.004072	0.279299
-18.948507	-2.052161	1.101056	0.004127	0.279008
-18.952196	-2.058898	1.106061	0.004128	0.278969
-18.918788	-2.078602	1.111066	0.004122	0.278898
-18.566712	-2.191598	1.116070	0.004056	0.278644
-18.842711	-2.142834	1.121075	0.004108	0.278636
-19.550485	-2.052641	1.126080	0.004239	0.278436
-19.507104	-2.079414	1.131085	0.004231	0.278337
-19.548673	-2.073993	1.136090	0.004239	0.278326
-20.148517	-2.015556	1.141094	0.004351	0.278062
-19.736354	-2.096848	1.146099	0.004274	0.278029
-19.447173	-2.170535	1.151104	0.004220	0.277919
-19.740345	-2.160917	1.156109	0.004275	0.277691
-19.584106	-2.193957	1.161114	0.004246	0.277666
-19.786817	-2.204582	1.166118	0.004284	0.277418
-20.320955	-2.116249	1.171123	0.004383	0.277372
-20.496607	-2.103303	1.176128	0.004416	0.277273
-20.249215	-2.191324	1.181133	0.004370	0.277048
-20.261147	-2.191241	1.186138	0.004372	0.277037
-20.639891	-2.166328	1.191142	0.004443	0.276807
-21.341130	-2.047856	1.196147	0.004573	0.276759
-21.313495	-2.063067	1.201152	0.004568	0.276706
-21.536521	-2.074290	1.206157	0.004610	0.276434
-21.406325	-2.101046	1.211162	0.004586	0.276418
-20.998014	-2.204497	1.216166	0.004510	0.276265
-21.458771	-2.150034	1.221171	0.004596	0.276111
-21.737507	-2.099382	1.226176	0.004648	0.276110
-22.049991	-2.096410	1.231181	0.004706	0.275828
-22.291118	-2.057460	1.236186	0.004751	0.275802
-22.139739	-2.097717	1.241190	0.004723	0.275734
-21.931605	-2.170818	1.246195	0.004684	0.275549
-21.844069	-2.187572	1.251200	0.004668	0.275544
-22.175268	-2.178136	1.256205	0.004729	0.275277
-23.198317	-2.002569	1.261210	0.004920	0.275222
-22.394798	-2.160349	1.266214	0.004770	0.275160
-22.417549	-2.207556	1.271219	0.004775	0.274890
-23.202656	-2.062493	1.276224	0.004921	0.274902
-23.008509	-2.136494	1.281229	0.004885	0.274697
-23.151750	-2.137448	1.286234	0.004911	0.274555
-23.165850	-2.137680	1.291238	0.004914	0.274540
-23.258261	-2.172121	1.296243	0.004931	0.274269
-23.175342	-2.188988	1.301248	0.004916	0.274260
-23.357254	-2.193058	1.306253	0.004950	0.274063
-24.011248	-2.099602	1.311258	0.005072	0.273928
-23.645399	-2.167441	1.316262	0.005004	0.273921
-23.671032	-2.218268	1.321267	0.005009	0.273627
-25.205649	-1.932456	1.326272	0.005294	0.273663
-24.428496	-2.098387	1.331277	0.005150	0.273532
-24.848538	-2.063102	1.336282	0.005228	0.273315
-24.584177	-2.109749	1.341286	0.005179	0.273322
-24.609567	-2.145869	1.346291	0.005183	0.273106
-24.847141	-2.120752	1.351296	0.005228	0.273010
-24.658124	-2.164283	1.356301	0.005193	0.272961
-25.322378	-2.097864	1.361306	0.005316	0.272672
-25.389387	-2.080836	1.366310	0.005329	0.272697
-25.152795	-2.153740	1.371315	0.005285	0.272538
-25.746296	-2.077554	1.376320	0.005395	0.272369
-25.812466	-2.062281	1.381325	0.005408	0.272386
-26.153163	-2.050580	1.386330	0.005471	0.272119
-26.338730	-2.026792	1.391334	0.005506	0.272066
-25.994010	-2.094541	1.396339	0.005442	0.272039
-26.177820	-2.113856	1.401344	0.005476	0.271757
-25.642799	-2.212540	1.406349	0.005376	0.271750
-26.233797	-2.141981	1.411354	0.005487	0.271553
-26.304494	-2.154700	1.416358	0.005500	0.271416
-26.681323	-2.081716	1.421363	0.005570	0.271440
-27.082560	-2.067487	1.426368	0.005645	0.271126
-26.307550	-2.212501	1.431373	0.005500	0.271104
-26.327019	-2.235484	1.436378	0.005504	0.270962
-27.307349	-2.085040	1.441382	0.005687	0.270813
-27.483619	-2.052614	1.446387	0.005720	0.270815
-27.318707	-2.125484	1.451392	0.005689	0.270585
-26.938591	-2.201263	1.456397	0.005618	0.270549
-27.281902	-2.164858	1.461402	0.005682	0.270410
-28.061076	-2.059072	1.466406	0.005827	0.270217
-27.535353	-2.158139	1.471411	0.005729	0.270198
-27.898488	-2.139077	1.476416	0.005797	0.269946
-28.281975	-2.078297	1.481421	0.005869	0.269898
-27.965104	-2.151583	1.486426	0.005810	0.269813
-28.169906	-2.163575	1.491430	0.005848	0.269549
-28.458559	-2.109101	1.496435	0.005902	0.269559
-28.475272	-2.140970	1.501440	0.005905	0.269371
-29.279562	-2.007560	1.506445	0.006054	0.269302
-28.941688	-2.074712	1.511450	0.005992	0.269271
-28.770570	-2.165271	1.516454	0.005960	0.268951
-28.443093	-2.229706	1.521459	0.005899	0.268924
-28.948080	-2.169298	1.526464	0.005993	0.268755
-29.479617	-2.096196	1.531469	0.006092	0.268628
-28.896787	-2.205308	1.536474	0.005984	0.268611
-29.290170	-2.191170	1.541478	0.006057	0.268301
-29.896027	-2.080129	1.546483	0.006170	0.268305
-29.569854	-2.166963	1.551488	0.006109	0.268156
-29.815890	-2.147838	1.556493	0.006155	0.268018
-30.144628	-2.089260	1.561498	0.006216	0.268011
-30.149769	-2.143270	1.566502	0.006217	0.267714
-30.026713	-2.175372	1.571507	0.006194	0.267661
-30.259175	-2.155329	1.576512	0.006238	0.267540
-30.829311	-2.083492	1.581517	0.006344	0.267367
-30.605700	-2.126597	1.586522	0.006302	0.267354
-30.422787	-2.207609	1.591526	0.006268	0.267095
-30.731152	-2.164826	1.596531	0.006326	0.267023
-30.620477	-2.203884	1.601536	0.006305	0.266920
-30.178621	-2.320056	1.606541	0.006223	0.266725
-30.838215	-2.202235	1.611546	0.006346	0.266713
-31.672496	-2.106121	1.616550	0.006501	0.266411
-31.087204	-2.214898	1.621555	0.006392	0.266398
-30.972707	-2.267897	1.626560	0.006371	0.266223
-31.572955	-2.181924	1.631565	0.006483	0.266096
-31.539493	-2.196738	1.636570	0.006477	0.266048
-31.452291	-2.263929	1.641574	0.006460	0.265769
-31.836100	-2.193586	1.646579	0.006532	0.265771
-31.817723	-2.234124	1.651584	0.006529	0.265568
-32.395118	-2.133586	1.656589	0.006636	0.265544
-32.455452	-2.140996	1.661594	0.006647	0.265443
-32.728046	-2.138852	1.666598	0.006698	0.265184
-32.804424	-2.122466	1.671603	0.006712	0.265197
-32.855779	-2.155951	1.676608	0.006722	0.264963
-33.164499	-2.116841	1.681613	0.006780	0.264870
-33.129035	-2.128985	1.686618	0.006773	0.264838
-32.994248	-2.208210	1.691622	0.006748	0.264539
-33.393612	-2.135719	1.696627	0.006822	0.264538
-33.273263	-2.191679	1.701632	0.006800	0.264351
-32.901914	-2.279546	1.706637	0.006731	0.264239
-33.333079	-2.215808	1.711642	0.006811	0.264158
-33.826909	-2.171225	1.716646	0.006903	0.263910
-33.723226	-2.190566	1.721651	0.006884	0.263907
-34.002346	-2.183664	1.726656	0.006936	0.263666
-34.411369	-2.119232	1.731661	0.007012	0.263611
-34.788963	-2.058089	1.736666	0.007082	0.263569
-34.573553	-2.147705	1.741670	0.007042	0.263292
-34.283876	-2.202333	1.746675	0.006989	0.263281
-34.875969	-2.125848	1.751680	0.007099	0.263109
-35.002496	-2.121409	1.756685	0.007122	0.263006
-34.823983	-2.161635	1.761690	0.007089	0.262963
-35.328553	-2.126710	1.766694	0.007183	0.262650
-35.244373	-2.140849	1.771699	0.007168	0.262656
-34.920474	-2.232699	1.776704	0.007107	0.262474
-35.576589	-2.135973	1.781709	0.007230	0.262349
-35.885064	-2.082396	1.786714	0.007287	0.262335
-35.780577	-2.155650	1.791718	0.007268	0.262035
-35.874244	-2.141876	1.796723	0.007285	0.262017
-36.323310	-2.079531	1.801728	0.007369	0.261909
-35.973151	-2.176269	1.806733	0.007304	0.261726
-35.938100	-2.184621	1.811738	0.007297	0.261715
-36.151968	-2.196201	1.816742	0.007337	0.261435
-36.549740	-2.131349	1.821747	0.007411	0.261394
-36.508261	-2.157483	1.826752	0.007403	0.261290
-36.610284	-2.175870	1.831757	0.007423	0.261085
-37.395028	-2.031708	1.836762	0.007569	0.261093
-37.242601	-2.100073	1.841766	0.007540	0.260867
-37.237523	-2.117204	1.846771	0.007539	0.260777
-38.005122	-1.976369	1.851776	0.007682	0.260783
-37.551398	-2.102054	1.856781	0.007598	0.260543
-37.548398	-2.105341	1.861786	0.007597	0.260528
-37.930173	-2.058407	1.866790	0.007669	0.260402
-38.074969	-2.069961	1.871795	0.007696	0.260191
-37.533315	-2.171760	1.876800	0.007595	0.260173
-38.124326	-2.105148	1.881805	0.007705	0.259945
-38.715864	-2.009429	1.886810	0.007815	0.259878
-38.445552	-2.066591	1.891814	0.007765	0.259833
-38.699638	-2.069461	1.896819	0.007812	0.259559
-38.942100	-2.027415	1.901824	0.007857	0.259547
-38.608334	-2.110998	1.906829	0.007795	0.259420
-38.977886	-2.071844	1.911834	0.007864	0.259263
-38.685009	-2.125605	1.916838	0.007810	0.259260
-38.849613	-2.151458	1.921843	0.007840	0.258947
-39.113421	-2.108858	1.926848	0.007889	0.258917
-38.849329	-2.179526	1.931853	0.007840	0.258790
-39.389337	-2.115316	1.936858	0.007941	0.258599
-38.775989	-2.228933	1.941862	0.007827	0.258588
-38.858204	-2.272327	1.946867	0.007842	0.258261
-39.870265	-2.084747	1.951872	0.008031	0.258280
-39.352703	-2.210237	1.956877	0.007934	0.258104
-39.738135	-2.160588	1.961882	0.008006	0.257988
-39.842907	-2.151507	1.966886	0.008026	0.257932
-40.346683	-2.107553	1.971891	0.008120	0.257664
-40.329292	-2.111644	1.976896	0.008116	0.257658
-40.354702	-2.141882	1.981901	0.008121	0.257462
-40.855775	-2.073013	1.986906	0.008214	0.257336
-40.233766	-2.196816	1.991910	0.008099	0.257276
-39.835291	-2.319514	1.996915	0.008025	0.256993
-40.252222	-2.266481	2.001920	0.008102	0.256864

-40.686853	-2.224419	2.011917	0.008183	0.256655
-41.161578	-2.186705	2.021914	0.008272	0.256380
-41.338373	-2.188613	2.031910	0.008305	0.256187
-41.267000	-2.221104	2.041907	0.008292	0.256076
-42.201381	-2.102181	2.051904	0.008466	0.255786
-41.368977	-2.259603	2.061901	0.008311	0.255752
-41.875011	-2.200881	2.071898	0.008405	0.255563
-42.374747	-2.116602	2.081894	0.008498	0.255524
-42.295098	-2.132175	2.091891	0.008483	0.255518
-42.417995	-2.146687	2.101888	0.008506	0.255308
-42.832315	-2.093716	2.111885	0.008584	0.255180
-42.897584	-2.081148	2.121882	0.008596	0.255184
-42.989212	-2.062197	2.131878	0.008613	0.255196
-43.180082	-2.026212	2.141875	0.008649	0.255203
-42.940394	-2.073073	2.151872	0.008604	0.255184
-43.033044	-2.054393	2.161869	0.008621	0.255194
-43.195370	-2.025092	2.171866	0.008652	0.255192
-43.006734	-2.059467	2.181862	0.008617	0.255191
-42.770924	-2.103536	2.191859	0.008573	0.255184
-42.472375	-2.160673	2.201856	0.008518	0.255167
-42.539619	-2.091559	2.211853	0.008530	0.255490
-42.657206	-2.064395	2.221850	0.008552	0.255522
-42.391728	-2.112443	2.231846	0.008503	0.255523
-42.870366	-2.022801	2.241843	0.008592	0.255537
-42.579138	-2.068026	2.251840	0.008538	0.255580
-42.638237	-2.021202	2.261837	0.008549	0.255784
-42.865234	-1.977979	2.271834	0.008591	0.255794
-42.608373	-2.007340	2.281830	0.008543	0.255892
-42.426487	-2.001708	2.291827	0.008510	0.256111
-42.518018	-1.984346	2.301824	0.008527	0.256114
-42.241906	-1.986228	2.311821	0.008476	0.256387
-42.159391	-1.996187	2.321818	0.008460	0.256415
-41.809309	-2.021558	2.331814	0.008395	0.256631
-41.994203	-1.965654	2.341811	0.008430	0.256756
-41.271649	-2.076816	2.351808	0.008295	0.256870
-41.026572	-2.095080	2.361805	0.008250	0.257018
-41.526331	-1.983773	2.371802	0.008343	0.257132
-40.605161	-2.112310	2.381798	0.008171	0.257352
-41.259272	-1.973319	2.391795	0.008293	0.257464
-40.865515	-2.006140	2.401792	0.008220	0.257681
-41.256513	-1.899357	2.411789	0.008293	0.257881
-41.031563	-1.913684	2.421786	0.008251	0.258030
-40.389194	-1.985283	2.431782	0.008132	0.258284
-40.330072	-1.976309	2.441779	0.008121	0.258394
-39.456184	-2.095960	2.451776	0.007958	0.258614
-39.822475	-2.001209	2.461773	0.008026	0.258770
-39.231360	-2.081402	2.471770	0.007916	0.258923
-39.531792	-1.980527	2.481766	0.007972	0.259181
-39.536326	-1.951476	2.491763	0.007973	0.259338
-38.959491	-2.017362	2.501760	0.007866	0.259555
-38.876498	-1.996163	2.511757	0.007851	0.259757
-38.927862	-1.955973	2.521754	0.007860	0.259929
-38.664978	-1.953353	2.531750	0.007812	0.260209
-38.461571	-1.950019	2.541747	0.007774	0.260433
-37.691097	-2.066094	2.551744	0.007630	0.260567
-38.398958	-1.895418	2.561741	0.007762	0.260799
-38.094608	-1.906591	2.571738	0.007706	0.261044
-37.663259	-1.952853	2.581734	0.007625	0.261222
-37.081953	-2.024159	2.591731	0.007517	0.261412
-36.976158	-1.988670	2.601728	0.007498	0.261715
-37.033425	-1.946450	2.611725	0.007508	0.261890
-36.419058	-2.030569	2.621722	0.007394	0.262043
-36.489153	-1.958998	2.631718	0.007407	0.262367
-36.046494	-2.003585	2.641715	0.007325	0.262565
-35.549134	-2.064504	2.651712	0.007233	0.262727
-35.575169	-2.008947	2.661709	0.007237	0.263007
-35.609794	-1.959400	2.671706	0.007244	0.263244
-35.618146	-1.919594	2.681702	0.007246	0.263454
-34.994202	-1.996000	2.691699	0.007130	0.263658
-34.709670	-1.997035	2.701696	0.007077	0.263936
-34.232521	-2.042121	2.711693	0.006988	0.264164
-34.396868	-1.975973	2.721690	0.007019	0.264362
-34.087064	-1.996936	2.731686	0.006961	0.264555
-33.679781	-2.013622	2.741683	0.006885	0.264869
-33.529861	-2.005376	2.751680	0.006857	0.265062
-33.316075	-2.008760	2.761677	0.006818	0.265256
-33.750461	-1.872832	2.771674	0.006899	0.265566
-33.440499	-1.883843	2.781670	0.006841	0.265813
-32.637583	-1.987668	2.791667	0.006692	0.266042
-32.228676	-2.028136	2.801664	0.006616	0.266226
-31.980025	-2.036899	2.811661	0.006569	0.266424
-31.804915	-2.007496	2.821658	0.006537	0.266756
-31.777196	-1.977772	2.831654	0.006532	0.266944
-31.652899	-1.959748	2.841651	0.006509	0.267164
-31.392186	-1.962631	2.851648	0.006460	0.267405
-31.226711	-1.939336	2.861645	0.006430	0.267693
-31.105856	-1.908652	2.871642	0.006407	0.267978
-30.690161	-1.944357	2.881638	0.006330	0.268193
-30.837207	-1.871240	2.891635	0.006357	0.268442
-30.739508	-1.838430	2.901632	0.006339	0.268715
-30.068801	-1.915221	2.911629	0.006214	0.268958
-29.808794	-1.904585	2.921626	0.006166	0.269269
-29.406529	-1.938773	2.931622	0.006091	0.269478
-29.355624	-1.902557	2.941619	0.006082	0.269722
-29.252769	-1.873407	2.951616	0.006063	0.269978
-28.663615	-1.934678	2.961613	0.005953	0.270223
-28.535343	-1.898443	2.971610	0.005929	0.270542
-28.695124	-1.829044	2.981606	0.005959	0.270757
-27.792456	-1.953208	2.991603	0.005791	0.270971
-27.671981	-1.932942	3.001600	0.005769	0.271195
-27.176260	-1.975015	3.011597	0.005677	0.271452
-27.057777	-1.945622	3.021594	0.005655	0.271723
-26.862921	-1.942413	3.031590	0.005619	0.271928
-26.425030	-1.980279	3.041587	0.005537	0.272150
-26.134619	-1.988951	3.051584	0.005483	0.272384
-25.709826	-2.014144	3.061581	0.005404	0.272660
-25.641823	-1.984710	3.071578	0.005392	0.272882
-25.398123	-1.990044	3.081574	0.005346	0.273088
-24.677547	-2.078537	3.091571	0.005212	0.273313
-24.825291	-2.003428	3.101568	0.005240	0.273568
-24.716830	-1.981290	3.111565	0.005220	0.273789
-24.238495	-2.034402	3.121562	0.005131	0.273968
-23.870652	-2.040706	3.131558	0.005062	0.274287
-23.975306	-1.981052	3.141555	0.005082	0.274501
-24.079323	-1.919566	3.151552	0.005101	0.274725
-23.582477	-1.965669	3.161549	0.005009	0.274958
-23.440438	-1.941783	3.171546	0.004983	0.275219
-22.777115	-2.006551	3.181542	0.004859	0.275512
-22.811472	-1.966096	3.191539	0.004866	0.275691
-22.597298	-1.967724	3.201536	0.004826	0.275887
-22.253005	-1.986110	3.211533	0.004762	0.276118
-21.886243	-1.998406	3.221530	0.004694	0.276403
-21.906557	-1.948266	3.231526	0.004698	0.276645
-21.757401	-1.931705	3.241523	0.004670	0.276873
-21.012791	-2.033192	3.251520	0.004531	0.277050
-20.786942	-2.011941	3.261517	0.004489	0.277375
-20.826370	-1.963495	3.271514	0.004497	0.277590
-20.581767	-1.964305	3.281510	0.004451	0.277817
-20.211315	-1.985295	3.291507	0.004383	0.278058
-19.479300	-2.070905	3.301504	0.004246	0.278305
-19.223888	-2.078504	3.311501	0.004199	0.278507
-19.335631	-2.019742	3.321498	0.004220	0.278706
-18.699575	-2.090406	3.331494	0.004101	0.278939
-19.108799	-1.958074	3.341491	0.004178	0.279239
-18.946718	-1.944951	3.351488	0.004148	0.279459
-18.846208	-1.918167	3.361485	0.004129	0.279692
-18.367913	-1.960886	3.371482	0.004040	0.279921
-18.036379	-1.960311	3.381478	0.003978	0.280235
-17.884021	-1.938487	3.391475	0.003950	0.280490
-17.732227	-1.926930	3.401472	0.003922	0.280691
-17.417955	-1.949574	3.411469	0.003863	0.280869
-16.817209	-2.012952	3.421466	0.003752	0.281105
-16.255815	-2.063967	3.431462	0.003647	0.281367
-16.400123	-1.997125	3.441459	0.003674	0.281575
-15.689762	-2.089273	3.451456	0.003542	0.281765
-15.671258	-2.040656	3.461453	0.003539	0.282032
-15.537354	-2.018810	3.471450	0.003514	0.282268
-15.240506	-2.034927	3.481446	0.003459	0.282462
-15.157825	-2.007855	3.491443	0.003443	0.282677
-14.623326	-2.038973	3.501440	0.003344	0.283015
-14.782855	-1.970448	3.511437	0.003374	0.283216
-14.348760	-2.014287	3.521434	0.003293	0.283395
-13.797610	-2.069864	3.531430	0.003191	0.283622
-13.851096	-2.002319	3.541427	0.003201	0.283917
-13.185554	-2.083566	3.551424	0.003077	0.284119
-13.156086	-2.052311	3.561421	0.003071	0.284305
-12.758217	-2.075504	3.571418	0.002997	0.284555
-12.525859	-2.071482	3.581414	0.002954	0.284789
-12.507272	-2.035069	3.591411	0.002951	0.284991
-11.859442	-2.111194	3.601408	0.002830	0.285202
-11.635568	-2.093500	3.611405	0.002789	0.285498
-11.239529	-2.140869	3.621402	0.002715	0.285622
-11.424702	-2.074362	3.631398	0.002750	0.285788
-10.687221	-2.147749	3.641395	0.002612	0.286095
-10.563445	-2.137260	3.651392	0.002590	0.286261
-10.529949	-2.109309	3.661389	0.002583	0.286433
-10.049915	-2.135368	3.671386	0.002494	0.286742
-9.858061	-2.135399	3.681382	0.002458	0.286917
-10.110658	-2.051677	3.691379	0.002506	0.287107
-9.854195	-2.045985	3.701376	0.002458	0.287370
-10.053489	-1.951985	3.711373	0.002495	0.287661
-9.570017	-1.986948	3.721370	0.002405	0.287926
-9.627194	-1.931965	3.731366	0.002416	0.288150
-9.150912	-1.972666	3.741363	0.002327	0.288380
-9.008175	-1.943502	3.751360	0.002301	0.288656
-8.852799	-1.919273	3.761357	0.002272	0.288918
-9.264193	-1.787022	3.771354	0.002348	0.289206
-8.631959	-1.848545	3.781350	0.002231	0.289472
-7.851137	-1.945909	3.791347	0.002086	0.289695
-7.720908	-1.918837	3.801344	0.002061	0.289948
-7.341812	-1.929642	3.811341	0.001991	0.290237
-6.956229	-1.948324	3.821338	0.001919	0.290493
-7.091095	-1.885888	3.831334	0.001944	0.290681
-7.568167	-1.748969	3.841331	0.002033	0.290931
-5.909630	-2.006408	3.851328	0.001725	0.291149
-4.868944	-2.139708	3.861325	0.001531	0.291426
-4.915127	-2.098636	3.871322	0.001540	0.291588
-5.023231	-2.040579	3.881318	0.001560	0.291778
-5.061034	-1.974037	3.891315	0.001567	0.292074
-6.635043	-1.640753	3.901312	0.001860	0.292307
-5.877417	-1.714684	3.911309	0.001719	0.292622
-4.549538	-1.899261	3.921306	0.001472	0.292902
-3.883887	-1.979796	3.931302	0.001348	0.293102
-3.837127	-1.937987	3.941299	0.001340	0.293349
-3.801602	-1.887255	3.951296	0.001333	0.293631
-3.910757	-1.825073	3.961293	0.001353	0.293839
-5.679951	-1.438413	3.971290	0.001683	0.294159
-4.402316	-1.605329	3.981286	0.001445	0.294480
-2.822874	-1.840434	3.991283	0.001151	0.294735
-2.050779	-1.940164	4.001280	0.001008	0.294933
-2.142399	-1.859742	4.011277	0.001025	0.295246
-2.625463	-1.719783	4.021274	0.001115	0.295501
-4.281701	-1.369986	4.031270	0.001423	0.295739
-3.937045	-1.364904	4.041267	0.001359	0.296070
-2.184888	-1.619892	4.051264	0.001033	0.296379
-1.211675	-1.734043	4.061261	0.000852	0.296685
-0.730107	-1.777134	4.071258	0.000762	0.296901
-0.768878	-1.730665	4.081254	0.000770	0.297093
-1.788250	-1.478103	4.091251	0.000959	0.297420
-4.412803	-0.918154	4.101248	0.001448	0.297823
-3.984449	-0.910746	4.111245	0.001368	0.298236
-1.441962	-1.297919	4.121242	0.000895	0.298599
0.138314	-1.523011	4.131238	0.000601	0.298900
0.465262	-1.528677	4.141235	0.000540	0.299159
-0.318121	-1.331385	4.151232	0.000686	0.299424
-2.661269	-0.833959	4.161229	0.001122	0.299770
-3.387073	-0.610441	4.171226	0.001257	0.300211
-2.381059	-0.698850	4.181222	0.001070	0.300666
0.168569	-1.094210	4.191219	0.000596	0.300992
2.185698	-1.402001	4.201216	0.000220	0.301274
1.482268	-1.220181	4.211213	0.000351	0.301533
0.156866	-0.909915	4.221210	0.000598	0.301865
-2.125458	-0.416770	4.231206	0.001023	0.302240
-1.962193	-0.341079	4.241203	0.000992	0.302744
-0.937688	-0.432497	4.251200	0.000802	0.303196
1.931545	-0.872589	4.261197	0.000268	0.303583
2.356564	-0.882747	4.271194	0.000189	0.303902
2.107694	-0.767699	4.281190	0.000235	0.304234
0.143406	-0.333934	4.291187	0.000601	0.304599
-1.679578	0.097170	4.301184	0.000940	0.305073
0.000000	-0.111746	4.311181	0.000627	0.305528

-0.410942	0.242631	4.316186	0.000704	0.306850
0.141176	0.706750	4.321190	0.000601	0.309500
2.523894	1.126408	4.326195	0.000157	0.313460
3.940690	2.018417	4.331200	-0.000108	0.318721
4.484332	3.358497	4.336205	-0.000210	0.325187
5.052000	4.998988	4.341210	-0.000316	0.332854
5.512946	6.947619	4.346214	-0.000403	0.341573
5.724432	9.262766	4.351219	-0.000444	0.351400
6.215748	11.823305	4.356224	-0.000537	0.362145
6.607899	14.723722	4.361229	-0.000612	0.373827
6.769153	17.995928	4.366234	-0.000644	0.386393
7.974009	21.405460	4.371238	-0.000871	0.399745
9.130389	25.184386	4.376243	-0.001089	0.413927
10.730724	29.229423	4.381248	-0.001389	0.428809
12.716701	33.562060	4.386253	-0.001762	0.444355
16.009934	38.031603	4.391258	-0.002378	0.460547
18.016153	43.105986	4.396262	-0.002755	0.477316
19.579047	48.626910	4.401267	-0.003049	0.494587
21.829634	54.388881	4.406272	-0.003472	0.512306
23.234743	60.633639	4.411277	-0.003738	0.530332
24.544734	67.229644	4.416282	-0.003986	0.548645
25.675196	74.175178	4.421286	-0.004201	0.567174
26.899220	81.427196	4.426291	-0.004433	0.585915
28.024804	88.969150	4.431296	-0.004648	0.604725
29.311732	96.761451	4.436301	-0.004892	0.623614
31.398134	104.670121	4.441306	-0.005286	0.642530
32.798545	112.949553	4.446310	-0.005552	0.661446
34.581941	121.371389	4.451315	-0.005890	0.680283
36.114583	130.041572	4.456320	-0.006181	0.699031
36.804309	139.028987	4.461325	-0.006315	0.717625
37.410897	148.184309	4.466330	-0.006434	0.736050
38.445334	157.390710	4.471334	-0.006632	0.754267
38.913684	166.814278	4.476339	-0.006726	0.772272
39.584037	176.282498	4.481344	-0.006856	0.790014
40.047238	185.859782	4.486349	-0.006949	0.807495
40.280072	195.539343	4.491354	-0.006999	0.824713
40.906599	205.174970	4.496358	-0.007121	0.841622
41.495767	214.844182	4.501363	-0.007237	0.858244
41.955536	224.546897	4.506368	-0.007329	0.874566
44.198833	233.930206	4.511373	-0.007753	0.890580
45.520234	243.527698	4.516378	-0.008005	0.906393
45.991783	253.234742	4.521382	-0.008099	0.921871
46.034292	263.019622	4.526387	-0.008114	0.937098
46.465113	272.684508	4.531392	-0.008200	0.952002
46.977943	282.279624	4.536397	-0.008302	0.966593
47.726962	291.819343	4.541402	-0.008447	0.980946
48.426330	301.334227	4.546406	-0.008584	0.995043
49.118471	310.773130	4.551411	-0.008719	1.008831
50.647716	320.041232	4.556416	-0.009010	1.022397
50.719255	329.528041	4.561421	-0.009029	1.035737
51.037065	338.905962	4.566426	-0.009094	1.048816
53.319086	347.886070	4.571430	-0.009525	1.061655
54.511747	357.064695	4.576435	-0.009753	1.074353
55.604446	366.189595	4.581440	-0.009962	1.086807
56.080239	375.395425	4.586445	-0.010057	1.099087
56.988111	384.474756	4.591450	-0.010232	1.111162
58.593979	393.376307	4.596454	-0.010537	1.123033
58.940259	402.503934	4.601459	-0.010607	1.134791
59.850780	411.460873	4.606464	-0.010782	1.146335
60.027903	420.513769	4.611469	-0.010821	1.157726
60.549009	429.434215	4.616474	-0.010924	1.168916
60.852658	438.346379	4.621478	-0.010986	1.179943
61.447598	447.175084	4.626483	-0.011103	1.190827
61.796869	455.996345	4.631488	-0.011173	1.201553
62.094868	464.799448	4.636493	-0.011235	1.212152
63.147787	473.441046	4.641498	-0.011436	1.222620
64.464453	482.025961	4.646502	-0.011687	1.232984
65.215850	490.682128	4.651507	-0.011832	1.243233
65.539817	499.395701	4.656512	-0.011898	1.253380
66.561731	507.936054	4.661517	-0.012094	1.263382
66.742629	516.643913	4.666522	-0.012134	1.273334
67.081980	525.247322	4.671526	-0.012202	1.283122
67.776754	533.788132	4.676531	-0.012337	1.292832
69.026935	542.215859	4.681536	-0.012575	1.302448
69.489550	550.821057	4.686541	-0.012667	1.312042
70.381732	559.276512	4.691546	-0.012839	1.321481
70.921900	567.762036	4.696550	-0.012945	1.330822
71.044337	576.322056	4.701555	-0.012973	1.340102
71.016388	584.865211	4.706560	-0.012973	1.349274
71.658423	593.258777	4.711565	-0.013098	1.358343
72.030045	601.706522	4.716570	-0.013173	1.367362
73.140286	609.992565	4.721574	-0.013385	1.376280
74.254445	618.315682	4.726579	-0.013598	1.385181
74.742664	626.753753	4.731584	-0.013694	1.394035
74.684749	635.232098	4.736589	-0.013689	1.402781
75.146993	643.609984	4.741594	-0.013780	1.411458
75.678932	651.954064	4.746598	-0.013885	1.420060
76.461551	660.273533	4.751603	-0.014036	1.428627
77.627546	668.535738	4.756608	-0.014258	1.437148
78.494279	676.805289	4.761613	-0.014425	1.445577
78.505771	685.283472	4.766618	-0.014433	1.454023
78.827302	693.618859	4.771622	-0.014498	1.462330
79.337596	701.968113	4.776627	-0.014598	1.470635
79.901923	710.269018	4.781632	-0.014709	1.478853
80.473176	718.537359	4.786637	-0.014821	1.486996
81.069719	726.829289	4.791642	-0.014937	1.495121
82.022552	735.037055	4.796646	-0.015120	1.503177
82.859073	743.294959	4.801651	-0.015281	1.511219
83.734581	751.516420	4.806656	-0.015449	1.519190
84.671028	759.733348	4.811661	-0.015629	1.527124
85.108758	768.081117	4.816666	-0.015716	1.535063
86.129218	776.284540	4.821670	-0.015911	1.542915
87.249027	784.486783	4.826675	-0.016125	1.550740
88.017470	792.741221	4.831680	-0.016273	1.558522
88.513252	801.015037	4.836685	-0.016371	1.566242
88.507765	809.411462	4.841690	-0.016375	1.573961
88.893724	817.690822	4.846694	-0.016453	1.581594
90.128619	825.813523	4.851699	-0.016688	1.589172
90.840851	834.046448	4.856704	-0.016826	1.596737
91.202752	842.320563	4.861709	-0.016898	1.604253
91.564210	850.616605	4.866714	-0.016971	1.611753
91.773758	858.893525	4.871718	-0.017015	1.619179
92.098951	867.140768	4.876723	-0.017081	1.626562
92.624086	875.389102	4.881728	-0.017184	1.633940
92.811802	883.610273	4.886733	-0.017225	1.641213
92.990083	891.868439	4.891738	-0.017263	1.648486
93.593010	900.039321	4.896742	-0.017381	1.655709
94.990070	908.055982	4.901747	-0.017646	1.662877
95.714529	916.244253	4.906752	-0.017786	1.670069
96.040617	924.482856	4.911757	-0.017852	1.677219
96.567940	932.682434	4.916762	-0.017956	1.684333
96.913359	940.910657	4.921766	-0.018025	1.691416
97.207287	949.134739	4.926771	-0.018085	1.698459
97.845403	957.294776	4.931776	-0.018210	1.705465
97.844818	965.589272	4.936781	-0.018215	1.712470
97.699725	973.847791	4.941786	-0.018193	1.719397
98.565833	981.886021	4.946790	-0.018360	1.726246
99.240700	990.056939	4.951795	-0.018491	1.733153
99.605235	998.239220	4.956800	-0.018564	1.740000
100.134523	1006.388223	4.961805	-0.018668	1.746815
100.548721	1014.589764	4.966810	-0.018750	1.753632
100.544990	1022.811831	4.971814	-0.018755	1.760385
101.244903	1030.911666	4.976819	-0.018890	1.767103
101.833700	1039.057155	4.981824	-0.019005	1.773817
101.940118	1047.274156	4.986829	-0.019030	1.780504
102.873557	1055.375718	4.991834	-0.019209	1.787176
103.820309	1063.492855	4.996838	-0.019391	1.793837
104.346860	1071.639835	5.001843	-0.019494	1.800444
104.583764	1079.829221	5.006848	-0.019543	1.807026
105.065840	1087.976973	5.011853	-0.019638	1.813580
105.755839	1096.085488	5.016858	-0.019772	1.820105
106.328131	1104.217890	5.021862	-0.019884	1.826612
106.533682	1112.443049	5.026867	-0.019928	1.833123
107.365804	1120.516858	5.031872	-0.020088	1.839568
107.662367	1128.687919	5.036877	-0.020148	1.846002
108.177250	1136.860020	5.041882	-0.020249	1.852441
109.071069	1144.922607	5.046886	-0.020421	1.858817
109.571272	1153.093508	5.051891	-0.020519	1.865208
110.220623	1161.219452	5.056896	-0.020646	1.871560
110.222738	1169.434904	5.061901	-0.020651	1.877883
111.081073	1177.485637	5.066906	-0.020816	1.884159
110.690854	1185.779984	5.071910	-0.020749	1.890455
110.906142	1193.940185	5.076915	-0.020794	1.896697
111.441216	1202.028567	5.081920	-0.020899	1.902902
111.665199	1210.200869	5.086925	-0.020946	1.909114
112.273975	1218.270501	5.091930	-0.021065	1.915273
112.564933	1226.398037	5.096934	-0.021124	1.921418
112.945284	1234.537712	5.101939	-0.021200	1.927564
113.821858	1242.587233	5.106944	-0.021369	1.933678
114.090725	1250.744342	5.111949	-0.021424	1.939785
114.392542	1258.916971	5.116954	-0.021485	1.945887
115.299961	1266.946991	5.121958	-0.021660	1.951933
115.435441	1275.101929	5.126963	-0.021690	1.957966
115.867344	1283.196385	5.131968	-0.021776	1.963968
116.152793	1291.341178	5.136973	-0.021834	1.969973
116.731807	1299.441003	5.141978	-0.021947	1.975959
116.935475	1307.569551	5.146982	-0.021990	1.981907
117.284090	1315.704484	5.151987	-0.022061	1.987857
118.237120	1323.749493	5.156992	-0.022243	1.993790
118.148337	1331.931992	5.161997	-0.022232	1.999692
118.365840	1340.084543	5.167002	-0.022278	2.005588
119.109515	1348.117524	5.172006	-0.022421	2.011436
119.900282	1356.180410	5.177011	-0.022574	2.017294
119.941720	1364.386644	5.182016	-0.022587	2.023158
120.694220	1372.418984	5.187021	-0.022732	2.028956
121.028211	1380.562826	5.192026	-0.022800	2.034772
121.409922	1388.639299	5.197030	-0.022876	2.040530
121.591176	1396.783322	5.202035	-0.022915	2.046297
121.845876	1404.923901	5.207040	-0.022968	2.052054
121.841876	1413.069508	5.212045	-0.022972	2.057771
122.556172	1421.113039	5.217050	-0.023110	2.063475
123.520685	1429.124116	5.222054	-0.023295	2.069165
123.712729	1437.280439	5.227059	-0.023336	2.074863
123.988415	1445.398025	5.232064	-0.023393	2.080526
124.365843	1453.485843	5.237069	-0.023468	2.086163
124.945305	1461.582896	5.242074	-0.023581	2.091812
124.897227	1469.765854	5.247078	-0.023578	2.097442
125.848149	1477.752534	5.252083	-0.023760	2.103021
126.671895	1485.794278	5.257088	-0.023918	2.108611
126.844081	1493.976627	5.262093	-0.023956	2.114217
127.558026	1501.997230	5.267098	-0.024094	2.119751
127.989262	1510.070858	5.272102	-0.024179	2.125280
128.117892	1518.246045	5.277107	-0.024209	2.130832
127.884927	1526.460422	5.282112	-0.024171	2.136362
128.191035	1534.505295	5.287117	-0.024233	2.141815
128.523882	1542.616580	5.292122	-0.024300	2.147302
128.737607	1550.716375	5.297126	-0.024345	2.152756
129.320203	1558.741407	5.302131	-0.024459	2.158181
130.242151	1566.720396	5.307136	-0.024636	2.163594
130.127763	1574.918715	5.312141	-0.024619	2.169040
130.829039	1582.962091	5.317146	-0.024755	2.174448
131.289573	1591.037284	5.322150	-0.024846	2.179840
131.427500	1599.172212	5.327155	-0.024877	2.185228
131.258717	1607.368876	5.332160	-0.024851	2.190614
131.262705	1615.470467	5.337165	-0.024857	2.195941
131.423310	1623.555925	5.342170	-0.024892	2.201259
131.575237	1631.620736	5.347174	-0.024926	2.206550
132.160412	1639.668816	5.352179	-0.025040	2.211857
132.692406	1647.705069	5.357184	-0.025144	2.217139
132.868340	1655.786151	5.362189	-0.025182	2.222405
133.481430	1663.837671	5.367194	-0.025301	2.227678
133.769007	1671.941280	5.372198	-0.025360	2.232944
134.207157	1680.004295	5.377203	-0.025447	2.238184
134.561045	1688.084770	5.382208	-0.025518	2.243415
135.176177	1696.136784	5.387213	-0.025638	2.248640
136.292796	1704.114569	5.392218	-0.025851	2.253850
136.595033	1712.243863	5.397222	-0.025912	2.259071
136.831250	1720.358025	5.402227	-0.025962	2.264265
137.301832	1728.470357	5.407232	-0.026054	2.269466
137.994322	1736.505240	5.412237	-0.026189	2.274626
138.333225	1744.585580	5.417242	-0.026257	2.279772
138.413733	1752.710910	5.422246	-0.026277	2.284912
138.708474	1760.811262	5.427251	-0.026337	2.290043
139.505911	1768.813426	5.432256	-0.026491	2.295144
139.900314	1776.860307	5.437261	-0.026570	2.300228
140.305344	1784.954762	5.442266	-0.026650	2.305330
140.659744	1793.046159	5.447270	-0.026721	2.310415
140.750980	1801.167807	5.452275	-0.026744	2.315485
141.042220	1809.254204	5.457280	-0.026803	2.320539
141.344833	1817.302239	5.462285	-0.026865	2.325559
141.965820	1825.365626	5.467290	-0.026986	2.330605
142.255319	1833.444002	5.472294	-0.027045	2.335621
142.829650	1841.491642	5.477299	-0.027157	2.340631
143.006548	1849.618803	5.482304	-0.027195	2.345646
143.248999	1857.684810	5.487309	-0.027245	2.350618
144.104486	1865.677488	5.492314	-0.027410	2.355586
144.573321	1873.719990	5.497318	-0.027502	2.360541
144.962444	1881.789517	5.502323	-0.027580	2.365496
145.166449	1889.941628	5.507328	-0.027623	2.370476
146.006265	1897.909487	5.512333	-0.027785	2.375385
146.050456	1906.073838	5.517338	-0.027798	2.380337
146.284566	1914.146691	5.522342	-0.027847	2.385240
146.952567	1922.168541	5.527347	-0.027977	2.390137
146.847590	1930.316487	5.532352	-0.027962	2.395037
147.786724	1938.239425	5.537357	-0.028142	2.399877
147.985167	1946.367421	5.542362	-0.028184	2.404769
148.212213	1954.460004	5.547366	-0.028232	2.409633
148.551065	1962.532179	5.552371	-0.028300	2.414484
148.570967	1970.667614	5.557376	-0.028309	2.419337
149.331086	1978.628537	5.562381	-0.028456	2.424135
149.640281	1986.738398	5.567386	-0.028519	2.428977
149.906079	1994.851710	5.572390	-0.028573	2.433807
150.270407	2002.883462	5.577395	-0.028646	2.438587
150.659294	2010.934582	5.582400	-0.028724	2.443371
150.214585	2019.110244	5.587405	-0.028647	2.448154
150.696826	2027.151189	5.592410	-0.028742	2.452921
150.907463	2035.208545	5.597414	-0.028786	2.457667
151.393381	2043.194400	5.602419	-0.028882	2.462383
152.057633	2051.232009	5.607424	-0.029011	2.467134
152.836258	2059.197430	5.612429	-0.029161	2.471842
153.011968	2067.315867	5.617434	-0.029199	2.476584
152.888729	2075.445882	5.622438	-0.029181	2.481301
153.319373	2083.475219	5.627443	-0.029266	2.485993
153.867204	2091.530334	5.632448	-0.029373	2.490700
153.569740	2099.699399	5.637453	-0.029323	2.495400
154.301776	2107.678393	5.642458	-0.029465	2.500058
155.158261	2115.621561	5.647462	-0.029629	2.504697
155.064331	2123.805882	5.652467	-0.029617	2.509394
155.372623	2131.878181	5.657472	-0.029680	2.514048
155.395811	2139.965444	5.662477	-0.029689	2.518681
155.648222	2148.004101	5.667482	-0.029742	2.523295
156.026766	2156.030956	5.672486	-0.029817	2.527903
156.462443	2164.066987	5.677491	-0.029904	2.532512
156.624812	2172.164922	5.682496	-0.029939	2.537127
156.939228	2180.194302	5.687501	-0.030003	2.541706
157.618995	2188.219088	5.692506	-0.030135	2.546301
158.187544	2196.252874	5.697510	-0.030246	2.550884
158.114034	2204.374166	5.702515	-0.030237	2.555462
158.918021	2212.364942	5.707520	-0.030392	2.560022
159.855302	2220.319306	5.712525	-0.030572	2.564562
160.166776	2228.436760	5.717530	-0.030635	2.569141
160.057081	2236.585621	5.722534	-0.030620	2.573699
160.975307	2244.527652	5.727539	-0.030796	2.578207
161.439334	2252.615013	5.732544	-0.030887	2.582755
161.491759	2260.728629	5.737549	-0.030902	2.587281
162.299298	2268.793975	5.742554	-0.031058	2.591826
162.154310	2276.981163	5.747558	-0.031036	2.596363
162.239864	2285.012107	5.752563	-0.031057	2.600821
163.058476	2292.933967	5.757568	-0.031215	2.605263
162.994829	2301.043930	5.762573	-0.031208	2.609740
163.616042	2309.065247	5.767578	-0.031329	2.614207
163.943800	2317.096250	5.772582	-0.031395	2.618652
164.435384	2325.109837	5.777587	-0.031492	2.623091
164.972960	2333.160606	5.782592	-0.031597	2.627546
164.639397	2341.321602	5.787597	-0.031541	2.631994
164.749054	2349.412247	5.792602	-0.031566	2.636426
165.301773	2357.373158	5.797606	-0.031674	2.640810
165.967317	2365.329923	5.802611	-0.031803	2.645192
166.574217	2373.376163	5.807616	-0.031922	2.649611
166.603695	2381.500369	5.812621	-0.031932	2.654027
167.190431	2389.536544	5.817626	-0.032047	2.658425
167.295588	2397.618001	5.822630	-0.032072	2.662807
167.796413	2405.641065	5.827635	-0.032170	2.667177
167.849346	2413.804380	5.832640	-0.032185	2.671586
168.596557	2421.729091	5.837645	-0.032329	2.675905
169.051828	2429.795724	5.842650	-0.032419	2.680274
169.368044	2437.808422	5.847654	-0.032483	2.684598
169.494189	2445.904041	5.852659	-0.032512	2.688947
169.377281	2454.055295	5.857664	-0.032496	2.693302
169.566928	2462.076581	5.862669	-0.032536	2.697601
170.038839	2470.074755	5.867674	-0.032629	2.701899
170.126455	2478.134290	5.872678	-0.032651	2.706198
170.713333	2486.148629	5.877683	-0.032765	2.710498
171.074926	2494.202090	5.882688	-0.032838	2.714798
171.419394	2502.219331	5.887693	-0.032907	2.719070
171.950408	2510.251124	5.892698	-0.033011	2.723356
171.729839	2518.408128	5.897702	-0.032975	2.727652
172.199219	2526.433470	5.902707	-0.033068	2.731917
173.093874	2534.399314	5.907712	-0.033240	2.736170
173.282160	2542.480414	5.912717	-0.033280	2.740432
173.395061	2550.561204	5.917722	-0.033306	2.744683
173.347531	2558.651087	5.922726	-0.033302	2.748922
173.718686	2566.719701	5.927731	-0.033377	2.753170
174.083132	2574.747405	5.932736	-0.033450	2.757389
174.795832	2582.689425	5.937741	-0.033588	2.761578
174.677830	2590.827470	5.942746	-0.033571	2.765812
174.765170	2598.879782	5.947750	-0.033592	2.770007
175.213612	2606.887889	5.952755	-0.033681	2.774196
175.396520	2614.952311	5.957760	-0.033720	2.778390
176.143950	2622.885385	5.962765	-0.033865	2.782545
176.672263	2630.933212	5.967770	-0.033968	2.786740
176.705209	2639.058236	5.972774	-0.033980	2.790937
177.086026	2647.083283	5.977779	-0.034056	2.795098
177.526030	2655.110559	5.982784	-0.034143	2.799258
177.645520	2663.157660	5.987789	-0.034170	2.803402
178.032498	2671.192880	5.992794	-0.034247	2.807550
178.462398	2679.240092	5.997798	-0.034333	2.811700
178.482925	2687.320735	6.002803	-0.034342	2.815837
179.009597	2695.335651	6.007808	-0.034445	2.819964
179.121745	2703.395895	6.012813	-0.034471	2.824084
179.552417	2711.439760	6.017818	-0.034556	2.828208
179.941103	2719.480809	6.022822	-0.034634	2.832323
180.334438	2727.480971	6.027827	-0.034712	2.836410
180.650293	2735.544298	6.032832	-0.034776	2.840519
180.880302	2743.553481	6.037837	-0.034824	2.844590
181.415860	2751.601028	6.042842	-0.034929	2.848692
181.756589	2759.664826	6.047846	-0.034998	2.852785
182.344144	2767.650282	6.052851	-0.035113	2.856847
182.556497	2775.749126	6.057856	-0.035157	2.860938
182.968164	2783.751290	6.062861	-0.035239	2.864987
183.445039	2791.801766	6.067866	-0.035333	2.869057
183.195390	2799.943833	6.072870	-0.035292	2.873126
183.438287	2807.946116	6.077875	-0.035342	2.877148
183.736093	2816.001632	6.082880	-0.035403	2.881193
184.059991	2824.005018	6.087885	-0.035468	2.885208
184.132554	2832.098782	6.092890	-0.035487	2.889249
184.564103	2840.124047	6.097894	-0.035573	2.893270
184.756325	2848.184435	6.102899	-0.035614	2.897289
185.339891	2856.194677	6.107904	-0.035728	2.901300
185.479269	2864.218122	6.112909	-0.035759	2.905286
186.044127	2872.258795	6.117914	-0.035869	2.909300
186.131033	2880.390048	6.122918	-0.035891	2.913326
186.454881	2888.389220	6.127923	-0.035956	2.917294
187.344417	2896.324616	6.132928	-0.036127	2.921257
187.229498	2904.423845	6.137933	-0.036111	2.925239
187.711444	2912.429268	6.142938	-0.036206	2.929203
187.367006	2920.575879	6.147942	-0.036147	2.933186
188.148145	2928.530301	6.152947	-0.036297	2.937130
189.126195	2936.472258	6.157952	-0.036484	2.941073
189.175697	2944.545306	6.162957	-0.036499	2.945025
189.327526	2952.694111	6.167962	-0.036532	2.949014
189.957081	2960.674947	6.172966	-0.036655	2.952941
190.077876	2968.734532	6.177971	-0.036683	2.956874
190.366557	2976.792386	6.182976	-0.036741	2.960810
190.840760	2984.760555	6.187981	-0.036835	2.964707
190.738361	2992.901929	6.192986	-0.036821	2.968652
191.243102	3000.899251	6.197990	-0.036920	2.972554
191.448941	3008.935212	6.202995	-0.036964	2.976454
192.126530	3016.904976	6.208000	-0.037095	2.980342
192.252962	3024.966993	6.213005	-0.037124	2.984240
192.856839	3033.019954	6.218010	-0.037241	2.988153
193.091375	3041.083280	6.223014	-0.037290	2.992047
193.354152	3049.124323	6.228019	-0.037344	2.995927
194.074837	3057.071580	6.233024	-0.037484	2.999780
194.172507	3065.136453	6.238029	-0.037507	3.003653
194.739901	3073.148610	6.243034	-0.037618	3.007519
194.864837	3081.256406	6.248038	-0.037647	3.011404
194.859124	3089.367711	6.253043	-0.037651	3.015278
195.368075	3097.359517	6.258048	-0.037751	3.019116
195.739928	3105.329744	6.263053	-0.037825	3.022933
196.038020	3113.400762	6.268058	-0.037886	3.026788
196.058766	3121.497052	6.273062	-0.037895	3.030637
196.399530	3129.490953	6.278067	-0.037963	3.034449
197.252858	3137.453044	6.283072	-0.038127	3.038266
197.536206	3145.488735	6.288077	-0.038185	3.042084
197.820912	3153.589371	6.293082	-0.038244	3.045929
197.859396	3161.632877	6.298086	-0.038256	3.049729
197.995504	3169.711355	6.303091	-0.038287	3.053546
198.456026	3177.741018	6.308096	-0.038378	3.057351
198.955139	3185.725790	6.313101	-0.038476	3.061132
199.469109	3193.735779	6.318106	-0.038576	3.064921
199.912060	3201.770633	6.323110	-0.038664	3.068713
199.849151	3209.901967	6.328115	-0.038658	3.072521
200.042339	3217.970885	6.333120	-0.038699	3.076308
200.351945	3225.922273	6.338125	-0.038762	3.080041
200.784734	3233.945059	6.343130	-0.038847	3.083808
200.740223	3242.010796	6.348134	-0.038844	3.087568
201.450511	3249.979526	6.353139	-0.038982	3.091314
201.841690	3258.056719	6.358144	-0.039060	3.095091
201.983311	3266.071977	6.363149	-0.039091	3.098822
202.637439	3274.045452	6.368154	-0.039218	3.102554
203.085688	3282.105055	6.373158	-0.039307	3.106311
203.251163	3290.183776	6.378163	-0.039343	3.110059
203.361745	3298.253576	6.383168	-0.039369	3.113796
203.988784	3306.189637	6.388173	-0.039491	3.117491
203.958490	3314.302635	6.393178	-0.039490	3.121233
203.631925	3322.384002	6.398182	-0.039435	3.124941
203.930688	3330.409263	6.403187	-0.039496	3.128649
204.402351	3338.452007	6.408192	-0.039589	3.132368
204.529017	3346.458803	6.413197	-0.039617	3.136050
205.078436	3354.471678	6.418202	-0.039725	3.139750
205.748450	3362.461126	6.423206	-0.039855	3.143440
205.910392	3370.497891	6.428211	-0.039890	3.147124
206.716085	3378.502793	6.433216	-0.040045	3.150819
206.460579	3386.630211	6.438221	-0.040003	3.154517
206.740046	3394.625735	6.443226	-0.040060	3.158174
206.879725	3402.687009	6.448230	-0.040091	3.161852
207.281195	3410.664645	6.453235	-0.040171	3.165498
208.043322	3418.669170	6.458240	-0.040318	3.169169
208.446143	3426.698665	6.463245	-0.040398	3.172830
208.715527	3434.764497	6.468250	-0.040454	3.176498
209.148577	3442.791367	6.473254	-0.040540	3.180151
208.772596	3450.896938	6.478259	-0.040475	3.183800
209.752446	3458.848512	6.483264	-0.040662	3.187434
209.902199	3466.939470	6.488269	-0.040696	3.191091
210.060164	3475.004334	6.493274	-0.040730	3.194732
209.942481	3483.047558	6.498278	-0.040713	3.198347
210.604353	3490.979389	6.503283	-0.040842	3.201942
210.932488	3499.029841	6.508288	-0.040908	3.205572
210.818537	3507.118181	6.513293	-0.040892	3.209196
210.549528	3515.233982	6.518298	-0.040847	3.212820
211.023837	3523.220618	6.523302	-0.040941	3.216415
211.124434	3531.220017	6.528307	-0.040965	3.219996
211.696013	3539.196735	6.533312	-0.041076	3.223583
212.369270	3547.150538	6.538317	-0.041207	3.227159
212.898137	3555.256922	6.543322	-0.041310	3.230794
213.292705	3563.275245	6.548326	-0.041389	3.234379
213.295320	3571.334834	6.553331	-0.041395	3.237962
213.858300	3579.332160	6.558336	-0.041505	3.241537
214.124959	3587.334127	6.563341	-0.041560	3.245098
214.694376	3595.356033	6.568346	-0.041671	3.248676
214.989252	3603.406480	6.573350	-0.041731	3.252251
215.345247	3611.465163	6.578355	-0.041802	3.255829
215.614214	3619.481607	6.583360	-0.041858	3.259380
215.671620	3627.523120	6.588365	-0.041874	3.262930
216.344406	3635.555153	6.593370	-0.042004	3.266496
216.248681	3643.642115	6.598374	-0.041991	3.270052
216.469661	3651.675103	6.603379	-0.042038	3.273593
217.013079	3659.688513	6.608384	-0.042144	3.277135
217.186955	3667.725025	6.613389	-0.042182	3.280668
217.435450	3675.707115	6.618394	-0.042233	3.284176
217.454571	3683.818835	6.623398	-0.042242	3.287728
218.212185	3691.746634	6.628403	-0.042388	3.291225
218.530964	3699.779165	6.633408	-0.042453	3.294747
218.656566	3707.831645	6.638413	-0.042481	3.298265
219.004629	3715.869661	6.643418	-0.042551	3.301783
219.235182	3723.895542	6.648422	-0.042599	3.305287
219.320410	3731.952577	6.653427	-0.042620	3.308795
219.918114	3739.953853	6.658432	-0.042737	3.312295
219.884493	3748.070566	6.663437	-0.042736	3.315816
219.943283	3756.072300	6.668442	-0.042752	3.319288
220.785665	3764.010540	6.673446	-0.042914	3.322759
221.260306	3772.007097	6.678451	-0.043008	3.326237
221.419740	3780.086737	6.683456	-0.043042	3.329735
222.244722	3788.044598	6.688461	-0.043201	3.333203
222.920363	3796.091821	6.693466	-0.043332	3.336700
223.041497	3804.174664	6.698470	-0.043360	3.340187
222.777904	3812.243552	6.703475	-0.043316	3.343649
223.274480	3820.283156	6.708480	-0.043414	3.347125
223.838843	3828.259190	6.713485	-0.043524	3.350572
223.957708	3836.309202	6.718490	-0.043551	3.354030
224.020749	3844.372496	6.723494	-0.043568	3.357488
224.128063	3852.413991	6.728499	-0.043593	3.360935
225.168112	3860.299590	6.733504	-0.043792	3.364347
225.210792	3868.386853	6.738509	-0.043805	3.367804
225.609551	3876.461653	6.743514	-0.043885	3.371265
226.169165	3884.440120	6.748518	-0.043994	3.374688
226.551560	3892.474609	6.753523	-0.044071	3.378124
226.824283	3900.548254	6.758528	-0.044127	3.381570
227.185906	3908.521918	6.763533	-0.044199	3.384972
227.619864	3916.585084	6.768538	-0.044285	3.388412
227.736994	3924.703789	6.773542	-0.044312	3.391860
227.905688	3932.731309	6.778547	-0.044349	3.395268
228.069255	3940.756354	6.783552	-0.044384	3.398672
228.885210	3948.647386	6.788557	-0.044541	3.402039
228.973951	3956.733550	6.793562	-0.044563	3.405458
229.203802	3964.765568	6.798566	-0.044611	3.408856
229.364433	3972.828628	6.803571	-0.044646	3.412262
230.435075	3980.783501	6.808576	-0.044851	3.415651
230.502864	3988.822567	6.813581	-0.044869	3.419036
230.534544	3996.923951	6.818586	-0.044880	3.422443
230.945039	4004.909360	6.823590	-0.044961	3.425811
231.417202	4012.910313	6.828595	-0.045054	3.429184
231.801581	4020.991558	6.833600	-0.045131	3.432585
231.728107	4029.016271	6.838605	-0.045123	3.435942
232.045038	4037.026750	6.843610	-0.045187	3.439304
232.152205	4045.065640	6.848614	-0.045212	3.442667
232.538698	4053.089296	6.853619	-0.045289	3.446030
233.085602	4061.076261	6.858624	-0.045396	3.449380
233.492844	4069.100018	6.863629	-0.045477	3.452737
233.745046	4077.176059	6.868634	-0.045529	3.456107
234.111000	4085.192180	6.873638	-0.045603	3.459453
234.154427	4093.230626	6.878643	-0.045616	3.462794
234.740240	4101.253619	6.883648	-0.045730	3.466143
235.322355	4109.217909	6.888653	-0.045844	3.469465
235.612097	4117.264408	6.893658	-0.045903	3.472808
235.807093	4125.344605	6.898662	-0.045944	3.476158
236.259618	4133.290212	6.903667	-0.046034	3.479458
235.918793	4141.411234	6.908672	-0.045976	3.482801
236.165835	4149.382042	6.913677	-0.046027	3.486098
236.856584	4157.364272	6.918682	-0.046160	3.489411
236.826801	4165.466013	6.923686	-0.046160	3.492747
237.390692	4173.457427	6.928691	-0.046270	3.496053
237.724878	4181.522869	6.933696	-0.046338	3.499379
237.743872	4189.536033	6.938701	-0.046346	3.502671
238.363025	4197.584494	6.943706	-0.046467	3.505993
238.580983	4205.578911	6.948710	-0.046513	3.509277
238.920868	4213.588075	6.953715	-0.046581	3.512567
239.548649	4221.626521	6.958720	-0.046703	3.515876
239.952856	4229.581883	6.963725	-0.046784	3.519140
240.063791	4237.689441	6.968730	-0.046810	3.522454
240.453467	4245.709394	6.973734	-0.046887	3.525738
240.535086	4253.711988	6.978739	-0.046908	3.529002
241.089604	4261.776533	6.983744	-0.047016	3.532303
241.118976	4269.803639	6.988749	-0.047027	3.535570
241.519323	4277.814085	6.993754	-0.047106	3.538838
241.881168	4285.836639	6.998758	-0.047179	3.542107
242.435323	4293.802689	7.003763	-0.047287	3.545355
242.599920	4301.900257	7.008768	-0.047323	3.548642
242.912594	4309.981728	7.013773	-0.047387	3.551924
243.416582	4317.992117	7.018778	-0.047486	3.555180
243.810555	4325.952009	7.023782	-0.047564	3.558409
243.787810	4334.019076	7.028787	-0.047565	3.561666
244.128474	4342.052800	7.033792	-0.047634	3.564917
243.927622	4350.085386	7.038797	-0.047602	3.568148
244.063504	4358.101312	7.043802	-0.047632	3.571380
244.475639	4366.104556	7.048806	-0.047714	3.574612
244.769795	4374.102335	7.053811	-0.047774	3.577836
245.494625	4382.130452	7.058816	-0.047914	3.581081
245.346746	4390.148053	7.063821	-0.047892	3.584294
246.002411	4398.169047	7.068826	-0.048019	3.587528
246.491677	4406.216187	7.073830	-0.048115	3.590765
246.534783	4414.211757	7.078835	-0.048128	3.593966
247.051057	4422.252184	7.083840	-0.048230	3.597195
247.217693	4430.268754	7.088845	-0.048266	3.600402
247.499339	4438.262967	7.093850	-0.048324	3.603600
247.822665	4446.347542	7.098854	-0.048389	3.606833
247.938752	4454.420171	7.103859	-0.048416	3.610051
248.440443	4462.413087	7.108864	-0.048514	3.613247
248.704543	4470.435303	7.113869	-0.048569	3.616444
248.904135	4478.452124	7.118874	-0.048611	3.619634
249.320876	4486.464346	7.123878	-0.048694	3.622826
249.727685	4494.484547	7.128883	-0.048775	3.626018
250.429740	4502.470273	7.133888	-0.048911	3.629202
250.553149	4510.561658	7.138893	-0.048939	3.632408
250.607883	4518.610674	7.143898	-0.048954	3.635593
250.790504	4526.596000	7.148902	-0.048993	3.638753
251.262472	4534.578055	7.153907	-0.049086	3.641918
251.690997	4542.576690	7.158912	-0.049171	3.645085
251.908171	4550.622798	7.163917	-0.049217	3.648262
251.975936	4558.728610	7.168922	-0.049235	3.651455
252.219155	4566.736318	7.173926	-0.049285	3.654612
252.764779	4574.669455	7.178931	-0.049392	3.657746
253.289079	4582.759864	7.183936	-0.049495	3.660937
253.603244	4590.714628	7.188941	-0.049559	3.664067
253.921819	4598.801914	7.193946	-0.049623	3.667246
254.426877	4606.813259	7.198950	-0.049722	3.670398
254.689231	4614.825371	7.203955	-0.049776	3.673540
254.990381	4622.943239	7.208960	-0.049838	3.676723
255.719815	4630.808565	7.213965	-0.049979	3.679815
256.118904	4638.849134	7.218970	-0.050058	3.682964
256.667278	4646.902577	7.223974	-0.050165	3.686120
256.455074	4654.952531	7.228979	-0.050131	3.689251
256.637064	4663.043395	7.233984	-0.050170	3.692405
256.865218	4671.036164	7.238989	-0.050218	3.695521
257.387912	4679.023904	7.243994	-0.050320	3.698639
257.572636	4687.089673	7.248998	-0.050360	3.701776
257.770245	4695.081814	7.254003	-0.050402	3.704882
257.913939	4703.178633	7.259008	-0.050434	3.708024
258.300674	4711.178256	7.264013	-0.050511	3.711133
258.584796	4719.235991	7.269018	-0.050569	3.714259
259.188358	4727.218034	7.274022	-0.050687	3.717361
259.029054	4735.243821	7.279027	-0.050662	3.720458
259.511824	4743.223296	7.284032	-0.050757	3.723550
260.166877	4751.209617	7.289037	-0.050884	3.726647
260.017850	4759.315656	7.294042	-0.050862	3.729767
259.966864	4767.367659	7.299046	-0.050858	3.732867
260.497365	4775.310446	7.304051	-0.050961	3.735936
260.711732	4783.365080	7.309056	-0.051007	3.739037
260.806770	4791.365942	7.314061	-0.051029	3.742113
260.799803	4799.393870	7.319066	-0.051033	3.745194
261.283798	4807.442356	7.324070	-0.051129	3.748292
261.630569	4815.452746	7.329075	-0.051198	3.751370
262.177259	4823.426056	7.334080	-0.051305	3.754436
262.235135	4831.490448	7.339085	-0.051321	3.757522
263.306056	4839.395621	7.344090	-0.051526	3.760569
263.899832	4847.373981	7.349094	-0.051642	3.763630
264.006942	4855.488971	7.354099	-0.051667	3.766729
263.973532	4863.608918	7.359104	-0.051666	3.769824
264.060312	4871.611540	7.364109	-0.051687	3.772874
264.449924	4879.664868	7.369114	-0.051765	3.775949
264.987587	4887.604812	7.374118	-0.051870	3.778981
265.290523	4895.616969	7.379123	-0.051932	3.782033
265.569509	4903.667662	7.384128	-0.051989	3.785096
266.143260	4911.678755	7.389133	-0.052101	3.788149
266.241060	4919.758922	7.394138	-0.052124	3.791214
266.727450	4927.729399	7.399142	-0.052220	3.794244
266.955579	4935.766881	7.404147	-0.052268	3.797292
267.747162	4943.720296	7.409152	-0.052420	3.800317
267.818573	4951.757381	7.414157	-0.052439	3.803356
267.915719	4959.837421	7.419162	-0.052462	3.806408
268.201666	4967.860399	7.424166	-0.052520	3.809441
267.833123	4975.959258	7.429171	-0.052457	3.812486
268.439470	4983.916191	7.434176	-0.052575	3.815496
268.615837	4991.929547	7.439181	-0.052613	3.818516
269.035467	4999.969667	7.444186	-0.052696	3.821549
269.223428	5007.948710	7.449190	-0.052737	3.824551
269.097132	5016.065092	7.454195	-0.052718	3.827595
269.521273	5024.088685	7.459200	-0.052802	3.830614
269.834588	5032.024519	7.464205	-0.052866	3.833596
270.679926	5040.053791	7.469210	-0.053028	3.836622
270.682763	5048.057388	7.474214	-0.053034	3.839617
270.866782	5056.077535	7.479219	-0.053074	3.842620
271.037877	5064.152441	7.484224	-0.053111	3.845641
271.114015	5072.186588	7.489229	-0.053130	3.848642
271.585040	5080.213412	7.494234	-0.053223	3.851647
271.846109	5088.195980	7.499238	-0.053277	3.854628
271.720534	5096.285886	7.504243	-0.053259	3.857638
272.312364	5104.273849	7.509248	-0.053374	3.860624
272.260975	5112.253737	7.514253	-0.053370	3.863590
272.919981	5120.270780	7.519258	-0.053497	3.866583
273.585154	5128.269586	7.524262	-0.053626	3.869567
273.727099	5136.461834	7.529267	-0.053658	3.872610
273.789743	5144.504146	7.534272	-0.053675	3.875593
274.259140	5152.419424	7.539277	-0.053768	3.878535
274.058854	5160.462729	7.544282	-0.053735	3.881508
274.388717	5168.378729	7.549286	-0.053802	3.884442
274.872689	5176.403857	7.554291	-0.053897	3.887418
275.608688	5184.407035	7.559296	-0.054039	3.890389
275.871802	5192.419019	7.564301	-0.054094	3.893351
276.000433	5200.545408	7.569306	-0.054123	3.896350
276.343155	5208.492631	7.574310	-0.054192	3.899285
276.130764	5216.566186	7.579315	-0.054157	3.902253
276.097651	5224.601256	7.584320	-0.054156	3.905208
276.194587	5232.614124	7.589325	-0.054180	3.908155
276.928082	5240.568992	7.594330	-0.054321	3.911092
277.187258	5248.613517	7.599334	-0.054375	3.914050
277.724011	5256.618726	7.604339	-0.054480	3.916996
277.873502	5264.661089	7.609344	-0.054513	3.919947
278.479978	5272.588917	7.614349	-0.054631	3.922862
278.431720	5280.714631	7.619354	-0.054627	3.925834
278.714672	5288.702598	7.624358	-0.054685	3.928760
279.529180	5296.662719	7.629363	-0.054842	3.931684
279.480307	5304.776997	7.634368	-0.054838	3.934646
279.774889	5312.795557	7.639373	-0.054898	3.937577
280.279216	5320.791330	7.644378	-0.054997	3.940501
280.387305	5328.828362	7.649382	-0.055023	3.943431
280.404239	5336.906159	7.654387	-0.055031	3.946372
280.495764	5344.960401	7.659392	-0.055053	3.949303
281.147974	5352.890566	7.664397	-0.055180	3.952197
281.061591	5360.958239	7.669402	-0.055169	3.955126
281.614157	5368.914196	7.674406	-0.055277	3.958023
281.470681	5377.006192	7.679411	-0.055255	3.960955
281.833628	5384.976033	7.684416	-0.055328	3.963850
282.508356	5392.917226	7.689421	-0.055459	3.966738
282.662681	5400.985483	7.694426	-0.055493	3.969660
283.025312	5409.060606	7.699430	-0.055566	3.972586
283.272163	5417.055965	7.704435	-0.055617	3.975479
283.987062	5425.024602	7.709440	-0.055755	3.978369
284.056038	5433.121188	7.714445	-0.055773	3.981291
284.307905	5441.045853	7.719450	-0.055825	3.984152
284.823984	5449.142014	7.724454	-0.055926	3.987078
285.095032	5457.162572	7.729459	-0.055982	3.989970
285.509488	5465.221192	7.734464	-0.056064	3.992876
285.416823	5473.257343	7.739469	-0.056052	3.995763
285.870678	5481.174745	7.744474	-0.056142	3.998615
286.126554	5489.241478	7.749478	-0.056195	4.001514
286.194507	5497.203844	7.754483	-0.056213	4.004371
286.726485	5505.248363	7.759488	-0.056317	4.007263
286.863873	5513.305380	7.764493	-0.056348	4.010151
286.853415	5521.372617	7.769498	-0.056351	4.013038
286.785369	5529.448367	7.774502	-0.056343	4.015925
286.960623	5537.412796	7.779507	-0.056381	4.018774
287.739723	5545.399473	7.784512	-0.056531	4.021639
287.765436	5553.371941	7.789517	-0.056541	4.024485
288.121885	5561.424147	7.794522	-0.056613	4.027362
288.626383	5569.430772	7.799526	-0.056712	4.030223
288.694064	5577.515908	7.804531	-0.056730	4.033103
289.309515	5585.559097	7.809536	-0.056850	4.035975
289.601430	5593.493835	7.814541	-0.056909	4.038801
289.622791	5601.549313	7.819546	-0.056918	4.041664
290.170801	5609.497126	7.824550	-0.057025	4.044495
290.438988	5617.496717	7.829555	-0.057081	4.047337
290.846504	5625.539886	7.834560	-0.057162	4.050195
290.874552	5633.578424	7.839565	-0.057172	4.053044
291.416810	5641.590222	7.844570	-0.057278	4.055889
292.043415	5649.567981	7.849574	-0.057400	4.058721
291.985310	5657.647808	7.854579	-0.057394	4.061577
292.059509	5665.659472	7.859584	-0.057413	4.064409
292.662157	5673.685681	7.864589	-0.057531	4.067251
292.423090	5681.783331	7.869594	-0.057492	4.070105
292.792270	5689.798411	7.874598	-0.057565	4.072936
293.112269	5697.755736	7.879603	-0.057630	4.075744
293.280515	5705.783702	7.884608	-0.057667	4.078573
293.368576	5713.854454	7.889613	-0.057688	4.081414
293.695159	5721.764457	7.894618	-0.057754	4.084200
293.762017	5729.890041	7.899622	-0.057772	4.087055
293.596183	5737.887856	7.904627	-0.057746	4.089861
293.419561	5745.981456	7.909632	-0.057719	4.092698
293.694800	5753.942517	7.914637	-0.057775	4.095493
294.156515	5761.889859	7.919642	-0.057866	4.098284
294.511589	5769.960483	7.924646	-0.057937	4.101115
294.906410	5777.925420	7.929651	-0.058016	4.103907
295.086765	5786.027049	7.934656	-0.058055	4.106742
295.250763	5794.003621	7.939661	-0.058091	4.109531
295.619038	5802.045444	7.944666	-0.058164	4.112344
295.518128	5810.101887	7.949670	-0.058151	4.115154
295.726539	5818.039502	7.954675	-0.058195	4.117924
296.049915	5826.087347	7.959680	-0.058260	4.120733
296.332340	5834.031220	7.964685	-0.058318	4.123502
297.123350	5842.058411	7.969690	-0.058470	4.126306
297.324531	5850.092901	7.974694	-0.058513	4.129103
297.523340	5858.101563	7.979699	-0.058555	4.131888
298.205504	5866.111405	7.984704	-0.058687	4.134679
297.935885	5874.232898	7.989709	-0.058642	4.137493
298.470943	5882.198397	7.994714	-0.058747	4.140262
298.937076	5890.208136	7.999718	-0.058839	4.143044
299.047300	5898.211701	8.004723	-0.058865	4.145817
299.487750	5906.209124	8.009728	-0.058952	4.148590
300.164685	5914.238436	8.014733	-0.059083	4.151376
300.410742	5922.213601	8.019738	-0.059134	4.154135
300.678268	5930.327220	8.024742	-0.059189	4.156940
301.227111	5938.224293	8.029747	-0.059296	4.159673
301.563368	5946.312090	8.034752	-0.059364	4.162466
301.717523	5954.271666	8.039757	-0.059398	4.165211
302.398562	5962.333480	8.044762	-0.059530	4.167997
302.492560	5970.422198	8.049766	-0.059553	4.170782
302.561193	5978.377452	8.054771	-0.059571	4.173519
302.881478	5986.522494	8.059776	-0.059636	4.176322
302.930636	5994.472765	8.064781	-0.059650	4.179054
302.993011	6002.546982	8.069786	-0.059667	4.181826
303.175226	6010.521320	8.074790	-0.059706	4.184564
303.265480	6018.608944	8.079795	-0.059728	4.187337
303.595083	6026.614340	8.084800	-0.059795	4.190084
303.520588	6034.683807	8.089805	-0.059786	4.192846
303.861262	6042.662138	8.094810	-0.059854	4.195579
304.674624	6050.538310	8.099814	-0.060011	4.198282
304.960458	6058.585909	8.104819	-0.060069	4.201035
304.694237	6066.627394	8.109824	-0.060025	4.203777
305.116088	6074.631679	8.114829	-0.060109	4.206513
305.632708	6082.580491	8.119834	-0.060210	4.209230
306.337386	6090.647549	8.124838	-0.060346	4.211987
306.095342	6098.682677	8.129843	-0.060307	4.214721
306.346948	6106.786559	8.134848	-0.060359	4.217481
306.757323	6114.723559	8.139853	-0.060440	4.220185
306.164226	6122.854581	8.144858	-0.060335	4.222942
307.051404	6130.748945	8.149862	-0.060505	4.225633
307.151295	6138.777910	8.154867	-0.060529	4.228360
307.554077	6146.833758	8.159872	-0.060609	4.231097
307.852979	6154.815373	8.164877	-0.060670	4.233806
308.075896	6162.867305	8.169882	-0.060717	4.236536
307.757451	6170.911940	8.174886	-0.060663	4.239256
308.255243	6178.873488	8.179891	-0.060761	4.241955
308.657015	6186.903319	8.184896	-0.060841	4.244675
308.748658	6194.878670	8.189901	-0.060863	4.247370
309.260411	6202.900888	8.194906	-0.060963	4.250085
309.757497	6210.952033	8.199910	-0.061061	4.252807
309.522164	6219.008365	8.204915	-0.061022	4.255521
309.538106	6227.025174	8.209920	-0.061031	4.258223
310.009637	6235.034483	8.214925	-0.061124	4.260926
310.542183	6242.969340	8.219930	-0.061228	4.263602
311.102265	6251.038577	8.224934	-0.061337	4.266322
310.859727	6259.079901	8.229939	-0.061297	4.269023
311.338347	6267.084917	8.234944	-0.061392	4.271717
311.207420	6275.161999	8.239949	-0.061372	4.274427
311.661665	6283.117635	8.244954	-0.061462	4.277101
311.969296	6291.158036	8.249958	-0.061525	4.279800
312.467489	6299.094836	8.254963	-0.061623	4.282464
312.641730	6307.139096	8.259968	-0.061660	4.285160
312.866073	6315.225368	8.264973	-0.061707	4.287868
312.886741	6323.239361	8.269978	-0.061716	4.290549
313.056929	6331.258963	8.274982	-0.061753	4.293231
313.439510	6339.240490	8.279987	-0.061829	4.295900
313.609331	6347.260012	8.284992	-0.061866	4.298579
313.775831	6355.308104	8.289997	-0.061902	4.301266
314.066190	6363.215636	8.295002	-0.061962	4.303905
314.669332	6371.325154	8.300006	-0.062079	4.306612
314.446776	6379.323786	8.305011	-0.062043	4.309274
315.011714	6387.337779	8.310016	-0.062153	4.311945
315.042592	6395.368879	8.315021	-0.062164	4.314617
315.839951	6403.288572	8.320026	-0.062318	4.317256
315.602625	6411.427770	8.325030	-0.062279	4.319957
315.971945	6419.358171	8.330035	-0.062353	4.322593
316.599757	6427.372768	8.335040	-0.062475	4.325257
316.380950	6435.423001	8.340045	-0.062439	4.327924
316.397970	6443.476081	8.345050	-0.062448	4.330592
316.866515	6451.485387	8.350054	-0.062540	4.333248
317.366868	6459.441466	8.355059	-0.062638	4.335885
317.613382	6467.503131	8.360064	-0.062689	4.338553
318.279619	6475.497496	8.365069	-0.062819	4.341200
318.625402	6483.453539	8.370074	-0.062888	4.343831
318.550285	6491.595659	8.375078	-0.062879	4.346518
318.437616	6499.583684	8.380083	-0.062864	4.349152
318.961076	6507.644255	8.385088	-0.062966	4.351814
318.918065	6515.722931	8.390093	-0.062964	4.354475
318.994160	6523.672013	8.395098	-0.062983	4.357094
319.670611	6531.600084	8.400102	-0.063114	4.359708
320.088582	6539.582631	8.405107	-0.063197	4.362336
320.086135	6547.636461	8.410112	-0.063202	4.364983
320.491484	6555.647281	8.415117	-0.063282	4.367617
320.618514	6563.691976	8.420122	-0.063311	4.370259
321.147413	6571.740576	8.425126	-0.063415	4.372904
320.832922	6579.740797	8.430131	-0.063361	4.375525
321.330147	6587.789559	8.435136	-0.063459	4.378165
321.428470	6595.825029	8.440141	-0.063483	4.380798
321.334351	6603.827380	8.445146	-0.063470	4.383416
321.591055	6611.889346	8.450150	-0.063523	4.386055
321.923081	6619.771322	8.455155	-0.063590	4.388634
322.654718	6627.830697	8.460160	-0.063732	4.391271
322.403976	6635.843065	8.465165	-0.063690	4.393886
322.755831	6643.897985	8.470170	-0.063761	4.396516
323.062847	6651.874481	8.475174	-0.063823	4.399119
322.852688	6659.916625	8.480179	-0.063789	4.401739
323.055539	6667.930644	8.485184	-0.063832	4.404351
323.449214	6675.945890	8.490189	-0.063911	4.406962
323.548042	6683.986948	8.495194	-0.063934	4.409579
324.160896	6692.076114	8.500198	-0.064054	4.412212
324.813687	6699.960114	8.505203	-0.064180	4.414778
325.122000	6708.060066	8.510208	-0.064243	4.417410
325.080960	6716.144318	8.515213	-0.064241	4.420034
325.813446	6724.073259	8.520218	-0.064382	4.422610
325.573125	6732.147546	8.525222	-0.064343	4.425226
326.073886	6740.136516	8.530227	-0.064441	4.427817
326.343223	6748.197049	8.535232	-0.064496	4.430428
326.196767	6756.234775	8.540237	-0.064474	4.433028
326.123492	6764.270146	8.545242	-0.064466	4.435626
326.339344	6772.252260	8.550246	-0.064511	4.438207
326.695357	6780.249381	8.555251	-0.064583	4.440792
327.306315	6788.206546	8.560256	-0.064701	4.443364
327.560407	6796.273992	8.565261	-0.064754	4.445968
327.602055	6804.281842	8.570266	-0.064767	4.448550
327.999148	6812.376032	8.575271	-0.064846	4.451160
327.606225	6820.389397	8.580275	-0.064778	4.453739
328.228279	6828.372381	8.585280	-0.064899	4.456312
328.917800	6836.286408	8.590285	-0.065033	4.458861
329.670887	6844.332525	8.595290	-0.065178	4.461451
329.922260	6852.330717	8.600295	-0.065230	4.464022
329.616252	6860.436993	8.605299	-0.065178	4.466624
330.019273	6868.439486	8.610304	-0.065258	4.469194
329.850034	6876.526854	8.615309	-0.065232	4.471787
330.190044	6884.470529	8.620314	-0.065301	4.474335
330.784776	6892.527493	8.625319	-0.065417	4.476919
330.550867	6900.536151	8.630323	-0.065378	4.479482
330.853169	6908.564633	8.635328	-0.065440	4.482052
331.503727	6916.442913	8.640333	-0.065566	4.484574
332.272298	6924.451389	8.645338	-0.065714	4.487137
332.503369	6932.539039	8.650343	-0.065762	4.489722
332.845742	6940.563540	8.655347	-0.065831	4.492285
333.038402	6948.607334	8.660352	-0.065872	4.494852
332.620786	6956.662220	8.665357	-0.065800	4.497419
332.874805	6964.638097	8.670362	-0.065852	4.499962
333.677411	6972.622949	8.675367	-0.066007	4.502508
333.677488	6980.599331	8.680371	-0.066012	4.505047
333.928294	6988.692226	8.685376	-0.066064	4.507623
334.264976	6996.666132	8.690381	-0.066132	4.510159
334.729318	7004.656047	8.695386	-0.066223	4.512700
334.796780	7012.728665	8.700391	-0.066241	4.515264
334.988468	7020.706212	8.705395	-0.066282	4.517797
335.068762	7028.750504	8.710400	-0.066302	4.520349
335.137247	7036.725631	8.715405	-0.066320	4.522878
335.601420	7044.733836	8.720410	-0.066412	4.525417
336.415302	7052.738386	8.725415	-0.066568	4.527955
336.481172	7060.742086	8.730419	-0.066586	4.530488
336.482008	7068.793359	8.735424	-0.066591	4.533035
337.176943	7076.807239	8.740429	-0.066726	4.535571
337.136619	7084.859174	8.745434	-0.066723	4.538115
337.589170	7092.879646	8.750439	-0.066813	4.540649
337.311818	7100.919959	8.755443	-0.066766	4.543186
337.877581	7108.922937	8.760448	-0.066877	4.545712
338.553890	7116.846486	8.765453	-0.067008	4.548212
338.480739	7124.936268	8.770458	-0.067000	4.550761
338.854517	7132.947742	8.775463	-0.067074	4.553285
339.232426	7140.924096	8.780467	-0.067150	4.555796
339.431013	7148.891445	8.785472	-0.067192	4.558303
339.541342	7156.992043	8.790477	-0.067218	4.560849
339.148740	7165.026211	8.795482	-0.067150	4.563373
339.664703	7173.005768	8.800487	-0.067251	4.565880
339.758122	7180.997700	8.805491	-0.067274	4.568389
340.173529	7189.091550	8.810496	-0.067356	4.570928
340.383701	7197.064849	8.815501	-0.067401	4.573428
340.413607	7205.111465	8.820506	-0.067411	4.575950
340.755839	7213.093896	8.825511	-0.067480	4.578450
340.988513	7221.135332	8.830515	-0.067529	4.580967
341.618687	7229.081284	8.835520	-0.067651	4.583454
341.808796	7237.157984	8.840525	-0.067692	4.585979
342.265097	7245.109942	8.845530	-0.067782	4.588465
342.843343	7253.161803	8.850535	-0.067895	4.590980
342.748152	7261.193448	8.855539	-0.067882	4.593487
342.859553	7269.242541	8.860544	-0.067908	4.595998
343.098010	7277.203392	8.865549	-0.067958	4.598480
342.927968	7285.228443	8.870554	-0.067931	4.600981
343.468458	7293.228960	8.875559	-0.068037	4.603473
343.660175	7301.250373	8.880563	-0.068078	4.605970
344.075472	7309.233276	8.885568	-0.068160	4.608454
344.151913	7317.323222	8.890573	-0.068180	4.610969
344.330351	7325.268574	8.895578	-0.068218	4.613438
344.794296	7333.342106	8.900583	-0.068310	4.615946
345.163524	7341.283656	8.905587	-0.068384	4.618412
345.211546	7349.431730	8.910592	-0.068398	4.620940
345.951103	7357.286581	8.915597	-0.068541	4.623376
345.748986	7365.426003	8.920602	-0.068508	4.625898
346.222494	7373.402125	8.925607	-0.068602	4.628369
346.430508	7381.467903	8.930611	-0.068646	4.630866
346.760912	7389.386533	8.935616	-0.068712	4.633316
346.666676	7397.489825	8.940621	-0.068700	4.635822
346.921101	7405.439440	8.945626	-0.068752	4.638279
347.120127	7413.520814	8.950631	-0.068795	4.640775
347.557722	7421.413240	8.955635	-0.068881	4.643212
347.931443	7429.530657	8.960640	-0.068956	4.645716
348.223979	7437.519986	8.965645	-0.069016	4.648180
348.243533	7445.597818	8.970650	-0.069025	4.650670
348.259878	7453.596869	8.975655	-0.069033	4.653134
348.153278	7461.602178	8.980659	-0.069018	4.655599
348.804095	7469.556188	8.985664	-0.069144	4.658047
348.946705	7477.610795	8.990669	-0.069176	4.660524
349.062999	7485.579316	8.995674	-0.069203	4.662974
349.453607	7493.617402	9.000679	-0.069281	4.665443
349.668501	7501.641394	9.005683	-0.069326	4.667907
349.631987	7509.742630	9.010688	-0.069325	4.670393
349.844946	7517.780360	9.015693	-0.069369	4.672859
350.420665	7525.678430	9.020698	-0.069482	4.675280
350.707319	7533.746373	9.025703	-0.069540	4.677752
351.243258	7541.684645	9.030707	-0.069645	4.680183
351.808282	7549.696705	9.035712	-0.069756	4.682635
351.809262	7557.721956	9.040717	-0.069761	4.685090
352.137930	7565.724751	9.045722	-0.069827	4.687537
352.406815	7573.779714	9.050727	-0.069883	4.689998
352.357885	7581.798148	9.055731	-0.069879	4.692447
352.501503	7589.804014	9.060736	-0.069911	4.694891
352.724916	7597.849194	9.065741	-0.069957	4.697346
353.219006	7605.753253	9.070746	-0.070054	4.699756
353.565922	7613.849506	9.075751	-0.070124	4.702223
354.021843	7621.797865	9.080755	-0.070214	4.704644
354.101969	7629.897596	9.085760	-0.070234	4.707110
354.358158	7637.912105	9.090765	-0.070287	4.709548
354.660568	7645.932120	9.095770	-0.070349	4.711987
354.977879	7653.946215	9.100775	-0.070413	4.714423
355.213978	7661.922032	9.105779	-0.070462	4.716846
355.358228	7669.949894	9.110784	-0.070494	4.719284
355.375227	7678.091360	9.115789	-0.070503	4.721755
355.432459	7685.988218	9.120794	-0.070518	4.724150
355.666701	7694.075543	9.125799	-0.070567	4.726602
355.918006	7702.003424	9.130803	-0.070619	4.729004
356.188640	7710.127328	9.135808	-0.070675	4.731464
356.514690	7718.107390	9.140813	-0.070741	4.733879
357.052058	7726.064170	9.145818	-0.070846	4.736286
357.406085	7734.097271	9.150823	-0.070917	4.738714
357.429220	7742.192225	9.155827	-0.070926	4.741161
357.870414	7750.104210	9.160832	-0.071014	4.743550
358.123439	7758.154443	9.165837	-0.071066	4.745981
358.060326	7766.235464	9.170842	-0.071060	4.748419
357.990202	7774.276051	9.175847	-0.071052	4.750845
358.291222	7782.236701	9.180851	-0.071113	4.753244
358.784760	7790.231062	9.185856	-0.071210	4.755652
358.825917	7798.281853	9.190861	-0.071223	4.758076
359.122858	7806.254948	9.195866	-0.071283	4.760476
359.613567	7814.256731	9.200871	-0.071380	4.762882
359.697820	7822.247671	9.205875	-0.071401	4.765284
359.338288	7830.414191	9.210880	-0.071339	4.767740
359.833481	7838.384917	9.215885	-0.071436	4.770133
360.184575	7846.342860	9.220890	-0.071507	4.772521
360.508354	7854.395197	9.225895	-0.071572	4.774937
360.528309	7862.388323	9.230899	-0.071581	4.777334
360.963059	7870.382412	9.235904	-0.071667	4.779729
361.168700	7878.437713	9.240909	-0.071711	4.782142
361.375577	7886.379354	9.245914	-0.071754	4.784520
361.293291	7894.526396	9.250919	-0.071744	4.786959
362.141987	7902.457103	9.255923	-0.071908	4.789329
361.963099	7910.539336	9.260928	-0.071879	4.791746
362.249112	7918.438617	9.265933	-0.071938	4.794106
362.498998	7926.547430	9.270938	-0.071990	4.796528
362.646896	7934.498175	9.275943	-0.072022	4.798901
362.779227	7942.592957	9.280947	-0.072052	4.801316
363.435931	7950.474189	9.285952	-0.072179	4.803665
363.584023	7958.594186	9.290957	-0.072212	4.806085
363.727186	7966.543258	9.295962	-0.072244	4.808453
364.196288	7974.617897	9.300967	-0.072337	4.810856
364.413284	7982.587546	9.305971	-0.072382	4.813227
364.343536	7990.169106	9.310976	-0.072374	4.815483
363.864075	7995.025137	9.315981	-0.072288	4.816929

364.317022	7997.527961	9.320986	-0.072374	4.817672
364.478093	7998.825923	9.325991	-0.072405	4.818057
364.920653	7999.259233	9.330995	-0.072487	4.818184
365.706338	8000.222268	9.336000	-0.072634	4.818467
365.751904	8000.328951	9.341005	-0.072643	4.818499
365.774359	8000.294589	9.346010	-0.072647	4.818488
365.593938	8000.394050	9.351015	-0.072613	4.818519
365.771530	8000.370164	9.356019	-0.072646	4.818511
366.374181	8000.296293	9.361024	-0.072758	4.818487
366.185001	8000.315817	9.366029	-0.072723	4.818493
366.188842	8000.352625	9.371034	-0.072724	4.818504
366.648237	8000.354562	9.376039	-0.072809	4.818503
366.400815	8000.344949	9.381043	-0.072763	4.818501
366.454539	8000.374022	9.386048	-0.072773	4.818509
366.675005	8000.361212	9.391053	-0.072814	4.818505
365.875326	8000.410385	9.396058	-0.072665	4.818522
366.044709	8000.478813	9.401063	-0.072697	4.818542
366.849508	8000.404497	9.406067	-0.072847	4.818517
366.468772	8000.444565	9.411072	-0.072776	4.818530
366.557341	8000.458350	9.416077	-0.072792	4.818534
366.636899	8000.486718	9.421082	-0.072807	4.818542
366.985375	8000.360087	9.426087	-0.072872	4.818503
366.892920	8000.409262	9.431091	-0.072854	4.818518
367.274876	8000.402814	9.436096	-0.072925	4.818515
366.992459	8000.458901	9.441101	-0.072873	4.818532
366.681704	8000.445289	9.446106	-0.072815	4.818530
367.169092	8000.436049	9.451111	-0.072906	4.818525
367.105254	8000.340664	9.456115	-0.072894	4.818497
366.947449	8000.445682	9.461120	-0.072864	4.818529
367.290995	8000.417714	9.466125	-0.072928	4.818519
367.423182	8000.432082	9.471130	-0.072953	4.818523
367.710816	8000.412820	9.476135	-0.073006	4.818516
367.623421	8000.401144	9.481139	-0.072990	4.818513
367.598892	8000.452278	9.486144	-0.072985	4.818528
368.211123	8000.380642	9.491149	-0.073099	4.818504
368.195877	8000.391988	9.496154	-0.073096	4.818508
368.505640	8000.375123	9.501159	-0.073154	4.818502
367.972728	8000.382693	9.506163	-0.073055	4.818506
368.248232	8000.401081	9.511168	-0.073106	4.818510
367.841123	8000.326309	9.516173	-0.073030	4.818490
367.551446	8000.488382	9.521178	-0.072976	4.818539
367.887735	8000.467670	9.526183	-0.073039	4.818531
367.831610	8000.354531	9.531187	-0.073028	4.818498
367.852278	8000.464038	9.536192	-0.073032	4.818531
368.005912	8000.473443	9.541197	-0.073061	4.818533
367.879220	8000.431831	9.546202	-0.073037	4.818521
368.416366	8000.412758	9.551207	-0.073137	4.818513
368.753833	8000.355301	9.556211	-0.073200	4.818495
368.505338	8000.420244	9.561216	-0.073153	4.818515
368.394339	8000.408251	9.566221	-0.073133	4.818512
368.311788	8000.412395	9.571226	-0.073117	4.818513
368.018937	8000.395869	9.576231	-0.073063	4.818510
368.414960	8000.389611	9.581235	-0.073136	4.818506
368.308982	8000.455411	9.586240	-0.073117	4.818526
368.070905	8000.507890	9.591245	-0.073072	4.818543
368.202016	8000.380450	9.596250	-0.073097	4.818504
367.959943	8000.437076	9.601255	-0.073051	4.818522
367.983249	8000.541368	9.606259	-0.073056	4.818553
368.367160	8000.373196	9.611264	-0.073127	4.818502
368.489510	8000.480915	9.616269	-0.073150	4.818533
368.466209	8000.420730	9.621274	-0.073146	4.818515
368.522119	8000.461389	9.626279	-0.073156	4.818527
368.640957	8000.419912	9.631283	-0.073178	4.818514
368.945732	8000.353614	9.636288	-0.073235	4.818493
368.292059	8000.484558	9.641293	-0.073113	4.818535
369.005312	8000.382765	9.646298	-0.073246	4.818502
368.982068	8000.463328	9.651303	-0.073241	4.818526
369.227003	8000.405683	9.656307	-0.073287	4.818508
369.035378	8000.352697	9.661312	-0.073251	4.818493
368.864061	8000.433378	9.666317	-0.073219	4.818517
368.620530	8000.457424	9.671322	-0.073174	4.818526
369.044117	8000.450487	9.676327	-0.073253	4.818522
368.799772	8000.437759	9.681331	-0.073207	4.818519
369.086017	8000.470998	9.686336	-0.073260	4.818528
368.748550	8000.424463	9.691341	-0.073197	4.818515
369.008298	8000.431088	9.696346	-0.073246	4.818516
369.137803	8000.418113	9.701351	-0.073270	4.818512
369.221318	8000.408724	9.706355	-0.073285	4.818509
369.390789	8000.332213	9.711360	-0.073317	4.818485
369.264326	8000.427150	9.716365	-0.073293	4.818514
369.148851	8000.361528	9.721370	-0.073272	4.818495
369.228964	8000.410914	9.726375	-0.073287	4.818509
368.734214	8000.421093	9.731379	-0.073194	4.818514
369.063009	8000.423390	9.736384	-0.073256	4.818514
369.350112	8000.406224	9.741389	-0.073309	4.818507
369.302507	8000.396130	9.746394	-0.073300	4.818505
369.583407	8000.414593	9.751399	-0.073352	4.818509
369.604481	8000.370756	9.756403	-0.073356	4.818496
369.610625	8000.416001	9.761408	-0.073357	4.818509
369.006753	8000.442574	9.766413	-0.073245	4.818520
369.266512	8000.460754	9.771418	-0.073293	4.818524
369.331916	8000.431166	9.776423	-0.073305	4.818515
369.060998	8000.450643	9.781427	-0.073255	4.818522
369.214272	8000.450591	9.786432	-0.073283	4.818521
369.224579	8000.406610	9.791437	-0.073285	4.818508
368.663613	8000.525140	9.796442	-0.073181	4.818546
368.949449	8000.480647	9.801447	-0.073234	4.818531
369.203529	8000.407369	9.806451	-0.073281	4.818508
369.468331	8000.384652	9.811456	-0.073330	4.818501
369.821131	8000.467101	9.816461	-0.073396	4.818524
369.681488	8000.457875	9.821466	-0.073370	4.818522
369.592858	8000.387360	9.826471	-0.073353	4.818501
369.236880	8000.449813	9.831475	-0.073287	4.818521
369.032450	8000.350440	9.836480	-0.073249	4.818492
368.992064	8000.343594	9.841485	-0.073241	4.818490
369.125842	8000.487180	9.846490	-0.073266	4.818532
369.272934	8000.419822	9.851495	-0.073294	4.818512
369.511073	8000.492332	9.856499	-0.073338	4.818532
369.551379	8000.380479	9.861504	-0.073345	4.818499
369.397442	8000.465595	9.866509	-0.073317	4.818525
369.244994	8000.484557	9.871514	-0.073288	4.818531
369.206919	8000.393713	9.876519	-0.073281	4.818504
369.462558	8000.413938	9.881523	-0.073329	4.818509
369.320385	8000.401527	9.886528	-0.073302	4.818506
370.123892	8000.441695	9.891533	-0.073452	4.818515
369.696661	8000.480085	9.896538	-0.073372	4.818528
369.726155	8000.373339	9.901543	-0.073378	4.818496
369.534775	8000.467407	9.906547	-0.073342	4.818525
369.424139	8000.434411	9.911552	-0.073321	4.818516
369.223559	8000.454830	9.916557	-0.073284	4.818522
369.180776	8000.466858	9.921562	-0.073276	4.818526
369.425107	8000.394500	9.926567	-0.073321	4.818504
369.663319	8000.438651	9.931571	-0.073366	4.818516
369.892714	8000.427014	9.936576	-0.073408	4.818512
369.336077	8000.476277	9.941581	-0.073305	4.818528
369.470022	8000.474916	9.946586	-0.073329	4.818527
369.594302	8000.330575	9.951591	-0.073352	4.818484
369.267780	8000.382920	9.956595	-0.073292	4.818501
369.517227	8000.368400	9.961600	-0.073338	4.818496
369.690373	8000.476803	9.966605	-0.073370	4.818527
369.970379	8000.436434	9.971610	-0.073422	4.818514
370.328972	8000.435983	9.976615	-0.073489	4.818512
370.526464	8000.392408	9.981619	-0.073526	4.818499
370.266212	8000.418329	9.986624	-0.073477	4.818507
370.355757	8000.430029	9.991629	-0.073494	4.818511
369.590100	8000.392461	9.996634	-0.073351	4.818502
369.849784	8000.402237	10.001639	-0.073400	4.818504
369.857884	8000.502129	10.006643	-0.073401	4.818534
369.762075	8000.409459	10.011648	-0.073383	4.818507
370.390474	8000.456737	10.016653	-0.073500	4.818518
370.355376	8000.458365	10.021658	-0.073494	4.818519
370.449579	8000.381894	10.026663	-0.073511	4.818496
370.402908	8000.456894	10.031667	-0.073502	4.818518
370.295270	8000.457549	10.036672	-0.073482	4.818519
370.368050	8000.476378	10.041677	-0.073496	4.818524
370.433101	8000.360652	10.046682	-0.073508	4.818490
370.473165	8000.459923	10.051687	-0.073515	4.818519
369.988615	8000.504897	10.056691	-0.073425	4.818534
370.120285	8000.404770	10.061696	-0.073449	4.818504
370.550667	8000.492463	10.066701	-0.073530	4.818528
370.500402	8000.381495	10.071706	-0.073520	4.818496
371.029120	8000.465255	10.076711	-0.073619	4.818518
370.938677	8000.433578	10.081715	-0.073602	4.818509
371.198142	8000.408691	10.086720	-0.073650	4.818501
370.746334	8000.395280	10.091725	-0.073566	4.818499
370.783876	8000.436745	10.096730	-0.073573	4.818511
371.060732	8000.473015	10.101735	-0.073624	4.818521
370.810958	8000.424497	10.106739	-0.073578	4.818507
370.418747	8000.389827	10.111744	-0.073505	4.818498
370.792920	8000.451559	10.116749	-0.073574	4.818515
370.334606	8000.410752	10.121754	-0.073489	4.818505
370.660745	8000.438227	10.126759	-0.073549	4.818512
370.503331	8000.446618	10.131763	-0.073520	4.818515
370.235925	8000.383160	10.136768	-0.073470	4.818497
370.358870	8000.492994	10.141773	-0.073493	4.818529
370.796681	8000.419027	10.146778	-0.073575	4.818506
370.878190	8000.399107	10.151783	-0.073590	4.818499
370.852437	8000.448128	10.156787	-0.073585	4.818514
371.060879	8000.449868	10.161792	-0.073624	4.818514
371.763924	8000.435129	10.166797	-0.073755	4.818507
371.504325	8000.379124	10.171802	-0.073706	4.818491
371.000706	8000.460606	10.176807	-0.073612	4.818517
370.543125	8000.464974	10.181811	-0.073527	4.818520
370.849430	8000.448068	10.186816	-0.073584	4.818514
370.465986	8000.378852	10.191821	-0.073513	4.818495
370.912951	8000.421602	10.196826	-0.073596	4.818506
371.514666	8000.405503	10.201831	-0.073708	4.818499
371.185778	8000.430503	10.206835	-0.073646	4.818507
371.270342	8000.443188	10.211840	-0.073662	4.818511
371.652342	8000.424145	10.216845	-0.073733	4.818504
371.225695	8000.415272	10.221850	-0.073654	4.818503
371.133292	8000.449744	10.226855	-0.073637	4.818513
371.226613	8000.393219	10.231859	-0.073654	4.818496
371.123691	8000.446458	10.236864	-0.073635	4.818512
371.113670	8000.357035	10.241869	-0.073633	4.818486
371.063997	8000.436197	10.246874	-0.073623	4.818510
371.015011	8000.431336	10.251879	-0.073614	4.818508
370.875356	8000.477779	10.256883	-0.073588	4.818523
370.894143	8000.481179	10.261888	-0.073592	4.818524
370.555002	8000.186724	10.266893	-0.073528	4.818438
371.122539	8000.377092	10.271898	-0.073634	4.818492
370.987871	8000.503433	10.276903	-0.073609	4.818530
371.310460	8000.370150	10.281907	-0.073669	4.818489
371.485816	8000.446026	10.286912	-0.073702	4.818511
371.754040	8000.441215	10.291917	-0.073752	4.818508
371.146637	8000.436221	10.296922	-0.073638	4.818509
371.437347	8000.466374	10.301927	-0.073692	4.818517
371.367710	8000.343590	10.306931	-0.073679	4.818481
371.341747	8000.437775	10.311936	-0.073675	4.818509
371.124046	8000.469518	10.316941	-0.073634	4.818519
371.454928	8000.437185	10.321946	-0.073696	4.818508
371.734808	8000.425177	10.326951	-0.073748	4.818504
371.388983	8000.416336	10.331955	-0.073683	4.818502
371.923406	8000.419295	10.336960	-0.073783	4.818501
371.689178	8000.420354	10.341965	-0.073739	4.818502
371.724833	8000.394568	10.346970	-0.073746	4.818495
371.644121	8000.419743	10.351975	-0.073730	4.818502
371.620130	8000.406813	10.356979	-0.073726	4.818499
371.740090	8000.418922	10.361984	-0.073748	4.818502
371.068719	8000.366853	10.366989	-0.073623	4.818489
371.418405	8000.388343	10.371994	-0.073688	4.818494
371.103689	8000.473406	10.376999	-0.073630	4.818521
371.174935	8000.384023	10.382003	-0.073643	4.818494
371.573969	8000.400922	10.387008	-0.073717	4.818497
371.702024	8000.413139	10.392013	-0.073741	4.818500
371.945464	8000.393290	10.397018	-0.073786	4.818493
372.117037	8000.412394	10.402023	-0.073818	4.818498
372.235337	8000.382464	10.407027	-0.073840	4.818489
372.045193	8000.430332	10.412032	-0.073805	4.818504
372.314887	8000.371969	10.417037	-0.073855	4.818486
371.882546	8000.395581	10.422042	-0.073774	4.818494
371.747794	8000.426335	10.427047	-0.073749	4.818504
371.213373	8000.445428	10.432051	-0.073650	4.818512
371.373154	8000.405550	10.437056	-0.073679	4.818499
371.375929	8000.447600	10.442061	-0.073680	4.818512
371.134594	8000.472723	10.447066	-0.073635	4.818520
372.049507	8000.450321	10.452071	-0.073805	4.818510
371.740099	8000.448270	10.457075	-0.073747	4.818511
371.931545	8000.365749	10.462080	-0.073783	4.818485
372.236526	8000.405549	10.467085	-0.073840	4.818496
371.933068	8000.387822	10.472090	-0.073783	4.818492
371.474372	8000.516123	10.477095	-0.073698	4.818532
371.412919	8000.375591	10.482099	-0.073686	4.818490
371.364420	8000.373887	10.487104	-0.073677	4.818490
371.700030	8000.494979	10.492109	-0.073740	4.818525
371.679561	8000.411717	10.497114	-0.073736	4.818500
371.861231	8000.442511	10.502119	-0.073770	4.818508
371.768132	8000.428655	10.507123	-0.073752	4.818505
371.617252	8000.374108	10.512128	-0.073724	4.818489
371.914902	8000.434817	10.517133	-0.073779	4.818506
371.905180	8000.454642	10.522138	-0.073778	4.818512
371.779172	8000.404629	10.527143	-0.073754	4.818497
371.743317	8000.450364	10.532147	-0.073747	4.818511
372.036390	8000.441685	10.537152	-0.073802	4.818507
372.221748	8000.429461	10.542157	-0.073836	4.818503
371.435727	8000.386357	10.547162	-0.073690	4.818493
371.655394	8000.467029	10.552167	-0.073731	4.818517
371.407050	8000.429033	10.557171	-0.073684	4.818506
371.470982	8000.505517	10.562176	-0.073696	4.818529
371.145805	8000.323635	10.567181	-0.073636	4.818476
371.262734	8000.408181	10.572186	-0.073657	4.818501
371.587203	8000.531224	10.577191	-0.073718	4.818536
371.509890	8000.393630	10.582195	-0.073703	4.818495
371.979355	8000.445088	10.587200	-0.073791	4.818509
371.775688	8000.404539	10.592205	-0.073753	4.818497
371.422396	8000.440766	10.597210	-0.073687	4.818510
371.859256	8000.481284	10.602215	-0.073768	4.818520
371.544746	8000.387778	10.607219	-0.073710	4.818493
371.626264	8000.455044	10.612224	-0.073725	4.818513
371.647290	8000.312465	10.617229	-0.073729	4.818471
371.733059	8000.490082	10.622234	-0.073745	4.818523
371.710669	8000.341669	10.627239	-0.073740	4.818479
372.115695	8000.427979	10.632243	-0.073816	4.818503
372.144968	8000.436771	10.637248	-0.073821	4.818506
372.473526	8000.417014	10.642253	-0.073882	4.818498
371.737602	8000.439706	10.647258	-0.073745	4.818508
372.027311	8000.434133	10.652263	-0.073799	4.818505
372.016264	8000.450788	10.657267	-0.073797	4.818510
371.818398	8000.361997	10.662272	-0.073760	4.818485
372.306609	8000.469381	10.667277	-0.073851	4.818515
371.761196	8000.455762	10.672282	-0.073749	4.818513
372.343796	8000.459369	10.677287	-0.073858	4.818512
372.259155	8000.386801	10.682291	-0.073842	4.818490
372.610318	8000.435625	10.687296	-0.073907	4.818503
372.296368	8000.444017	10.692301	-0.073849	4.818507
371.767671	8000.474740	10.697306	-0.073750	4.818518
371.964730	8000.375487	10.702311	-0.073787	4.818488
372.004639	8000.391775	10.707315	-0.073794	4.818493
372.104775	8000.454039	10.712320	-0.073813	4.818511
372.060585	8000.411426	10.717325	-0.073805	4.818498
371.622573	8000.363534	10.722330	-0.073723	4.818486
371.939157	8000.426598	10.727335	-0.073782	4.818503
371.731612	8000.438518	10.732339	-0.073743	4.818508
372.152672	8000.472522	10.737344	-0.073822	4.818516
372.511349	8000.395395	10.742349	-0.073888	4.818492
372.383401	8000.495568	10.747354	-0.073865	4.818522
372.164959	8000.349776	10.752359	-0.073824	4.818480
371.964697	8000.526712	10.757363	-0.073786	4.818533
371.700685	8000.399218	10.762368	-0.073737	4.818496
371.604321	8000.300234	10.767373	-0.073719	4.818467
371.968109	8000.499436	10.772378	-0.073787	4.818525
372.230322	8000.363241	10.777383	-0.073836	4.818483
372.469554	8000.445228	10.782387	-0.073880	4.818507
371.705593	8000.424477	10.787392	-0.073738	4.818504
372.074076	8000.547063	10.792397	-0.073807	4.818539
371.906592	8000.281156	10.797402	-0.073775	4.818460
372.180995	8000.284831	10.802407	-0.073826	4.818460
371.628769	8000.189192	10.807411	-0.073723	4.818434
371.548119	8000.263737	10.812416	-0.073708	4.818457
371.681136	8000.265516	10.817421	-0.073733	4.818457
371.433771	8000.389298	10.822426	-0.073687	4.818494
372.173158	8000.343533	10.827431	-0.073825	4.818478
372.128387	8000.474234	10.832435	-0.073816	4.818517
371.686667	8000.430492	10.837440	-0.073734	4.818506
371.985223	8000.434492	10.842445	-0.073789	4.818506
372.105131	8000.506475	10.847450	-0.073812	4.818526
371.947452	8000.350995	10.852455	-0.073782	4.818481
371.713955	8000.449753	10.857459	-0.073739	4.818511
372.163495	8000.490441	10.862464	-0.073822	4.818522
372.172675	8000.439089	10.867469	-0.073824	4.818506
372.170365	8000.496829	10.872474	-0.073824	4.818523
372.455708	8000.398760	10.877479	-0.073877	4.818493
372.493424	8000.412918	10.882483	-0.073884	4.818497
372.114776	8000.433047	10.887488	-0.073813	4.818505
372.355100	8000.442569	10.892493	-0.073858	4.818507
372.649730	8000.438114	10.897498	-0.073913	4.818504
372.450540	8000.465902	10.902503	-0.073876	4.818513
372.392006	8000.396835	10.907507	-0.073865	4.818493
372.341081	8000.429763	10.912512	-0.073855	4.818503
372.184476	8000.348877	10.917517	-0.073826	4.818479
372.777572	8000.452417	10.922522	-0.073936	4.818508
372.846461	8000.482751	10.927527	-0.073949	4.818517
373.400419	8000.413496	10.932531	-0.074052	4.818494
373.232333	8000.394430	10.937536	-0.074021	4.818489
373.363739	8000.429804	10.942541	-0.074045	4.818499
373.218216	8000.408940	10.947546	-0.074018	4.818493
373.216935	8000.412071	10.952551	-0.074018	4.818494
373.194000	8000.404407	10.957555	-0.074013	4.818492
372.945053	8000.471444	10.962560	-0.073967	4.818513
372.631010	8000.431513	10.967565	-0.073909	4.818502
372.422288	8000.405601	10.972570	-0.073870	4.818495
372.890182	8000.411873	10.977575	-0.073957	4.818495
373.365920	8000.467623	10.982579	-0.074045	4.818510
372.783619	8000.483968	10.987584	-0.073937	4.818517
373.500630	8000.438961	10.992589	-0.074070	4.818501
373.267558	8000.446335	10.997594	-0.074027	4.818504
373.112568	8000.450555	11.002599	-0.073998	4.818506
372.812105	8000.385595	11.007603	-0.073942	4.818488
372.893684	8000.472823	11.012608	-0.073957	4.818513
372.710749	8000.422045	11.017613	-0.073923	4.818499
372.803483	8000.428537	11.022618	-0.073940	4.818501
373.008340	8000.376658	11.027623	-0.073978	4.818484
373.004203	8000.492150	11.032627	-0.073977	4.818519
372.727139	8000.381284	11.037632	-0.073926	4.818487
372.728971	8000.483198	11.042637	-0.073926	4.818517
372.830274	8000.474049	11.047642	-0.073945	4.818514
373.217272	8000.426715	11.052647	-0.074017	4.818498
373.305633	8000.350163	11.057651	-0.074033	4.818475
373.459484	8000.409999	11.062656	-0.074062	4.818492
373.101699	8000.487131	11.067661	-0.073995	4.818517
373.160210	8000.458500	11.072666	-0.074006	4.818508
372.922846	8000.412244	11.077671	-0.073962	4.818495
372.948851	8000.478768	11.082675	-0.073967	4.818515
372.529518	8000.431122	11.087680	-0.073889	4.818502
372.909763	8000.471934	11.092685	-0.073959	4.818513
372.908986	8000.376329	11.097690	-0.073959	4.818485
373.046237	8000.463254	11.102695	-0.073985	4.818510
372.716463	8000.456726	11.107699	-0.073923	4.818509
372.826243	8000.398319	11.112704	-0.073944	4.818492
373.112309	8000.497745	11.117709	-0.073997	4.818520
372.885919	8000.407517	11.122714	-0.073955	4.818494
372.628436	8000.435573	11.127719	-0.073907	4.818503
372.712591	8000.430396	11.132723	-0.073922	4.818502
372.746744	8000.489676	11.137728	-0.073929	4.818519
373.178103	8000.470248	11.142733	-0.074009	4.818512
372.663868	8000.396118	11.147738	-0.073913	4.818492
373.078616	8000.466806	11.152743	-0.073990	4.818511
372.629035	8000.393543	11.157747	-0.073906	4.818491
372.561899	8000.514491	11.162752	-0.073894	4.818527
372.592980	8000.403557	11.167757	-0.073900	4.818494
372.374739	8000.477310	11.172762	-0.073859	4.818517
372.347351	8000.357189	11.177767	-0.073854	4.818481
372.357084	8000.290089	11.182771	-0.073855	4.818461
372.425633	8000.342475	11.187776	-0.073868	4.818477
372.340872	8000.319277	11.192781	-0.073852	4.818470
372.226835	8000.321946	11.197786	-0.073831	4.818471
372.666949	8000.428686	11.202791	-0.073913	4.818501
372.829813	8000.398303	11.207795	-0.073943	4.818492
372.652318	8000.485208	11.212800	-0.073910	4.818518
372.634964	8000.439802	11.217805	-0.073907	4.818505
372.672947	8000.415098	11.222810	-0.073914	4.818497
373.049061	8000.468460	11.227815	-0.073984	4.818512
372.836726	8000.404682	11.232819	-0.073944	4.818493
372.790000	8000.390396	11.237824	-0.073936	4.818489
373.159524	8000.402703	11.242829	-0.074004	4.818492
372.989557	8000.471850	11.247834	-0.073973	4.818513
373.333155	8000.489062	11.252839	-0.074037	4.818517
373.251769	8000.399728	11.257843	-0.074021	4.818490
373.275358	8000.363275	11.262848	-0.074026	4.818479
373.498923	8000.415643	11.267853	-0.074067	4.818494
373.467788	8000.407869	11.272858	-0.074061	4.818492
373.476573	8000.439497	11.277863	-0.074063	4.818501
373.559093	8000.437450	11.282867	-0.074078	4.818500
373.411527	8000.423911	11.287872	-0.074051	4.818497
373.502828	8000.442991	11.292877	-0.074068	4.818502
373.368364	8000.421224	11.297882	-0.074043	4.818496
373.753403	8000.409580	11.302887	-0.074114	4.818491
373.717489	8000.397540	11.307891	-0.074108	4.818488
374.064614	8000.327611	11.312896	-0.074172	4.818466
374.328008	8000.355303	11.317901	-0.074221	4.818473
373.860463	8000.399448	11.322906	-0.074134	4.818488
374.147193	8000.399091	11.327911	-0.074187	4.818487
374.238753	8000.374054	11.332915	-0.074204	4.818479
374.063084	8000.403208	11.337920	-0.074172	4.818488
373.537696	8000.453930	11.342925	-0.074074	4.818505
373.154295	8000.477145	11.347930	-0.074002	4.818514
373.759019	8000.327685	11.352935	-0.074115	4.818467
373.997490	8000.387607	11.357939	-0.074159	4.818484
373.822610	8000.408368	11.362944	-0.074127	4.818491
374.356251	8000.402921	11.367949	-0.074226	4.818487
374.161594	8000.400304	11.372954	-0.074190	4.818487
374.059360	8000.444100	11.377959	-0.074171	4.818500
374.215979	8000.424138	11.382963	-0.074200	4.818494
373.808002	8000.448073	11.387968	-0.074124	4.818502
373.583399	8000.453459	11.392973	-0.074082	4.818505
373.782740	8000.413061	11.397978	-0.074119	4.818492
374.230482	8000.421168	11.402983	-0.074202	4.818493
373.922638	8000.406528	11.407987	-0.074145	4.818490
373.983296	8000.430449	11.412992	-0.074156	4.818497
374.363418	8000.423993	11.417997	-0.074227	4.818493
373.855548	8000.395113	11.423002	-0.074132	4.818487
373.872659	8000.353321	11.428007	-0.074135	4.818474
373.775534	8000.411891	11.433011	-0.074117	4.818492
373.902105	8000.398879	11.438016	-0.074141	4.818487
373.978648	8000.442973	11.443021	-0.074155	4.818500
374.090394	8000.399299	11.448026	-0.074176	4.818487
374.123117	8000.462763	11.453031	-0.074182	4.818506
374.497276	8000.371138	11.458035	-0.074251	4.818477
374.376788	8000.383173	11.463040	-0.074229	4.818481
374.383252	8000.411620	11.468045	-0.074230	4.818489
374.491078	8000.350035	11.473050	-0.074250	4.818471
374.293795	8000.409362	11.478055	-0.074213	4.818489
374.532220	8000.325368	11.483059	-0.074258	4.818463
374.518487	8000.368251	11.488064	-0.074255	4.818476
374.215235	8000.404095	11.493069	-0.074199	4.818488
374.244903	8000.389783	11.498074	-0.074204	4.818483
374.382040	8000.449398	11.503079	-0.074230	4.818501
374.601380	8000.398764	11.508083	-0.074270	4.818485
374.457812	8000.395783	11.513088	-0.074244	4.818484
374.477929	8000.430715	11.518093	-0.074247	4.818495
374.160234	8000.401236	11.523098	-0.074188	4.818487
374.382460	8000.409468	11.528103	-0.074229	4.818489
374.090252	8000.441259	11.533107	-0.074175	4.818499
373.989051	8000.429392	11.538112	-0.074156	4.818496
374.084480	8000.451679	11.543117	-0.074174	4.818502
374.143798	8000.416756	11.548122	-0.074185	4.818492
374.175728	8000.474958	11.553127	-0.074191	4.818509
374.616094	8000.441998	11.558131	-0.074273	4.818497
374.365943	8000.403970	11.563136	-0.074226	4.818487
374.679407	8000.437589	11.568141	-0.074284	4.818496
374.461100	8000.403140	11.573146	-0.074244	4.818487
374.739084	8000.408969	11.578151	-0.074295	4.818487
374.561452	8000.400278	11.583155	-0.074262	4.818485
374.529054	8000.416648	11.588160	-0.074256	4.818490
374.705237	8000.435818	11.593165	-0.074289	4.818495
374.555908	8000.364477	11.598170	-0.074261	4.818475
374.595646	8000.444845	11.603175	-0.074268	4.818498
374.564420	8000.403453	11.608179	-0.074263	4.818486
374.303961	8000.413610	11.613184	-0.074214	4.818490
374.508660	8000.406900	11.618189	-0.074252	4.818487
374.581149	8000.396314	11.623194	-0.074266	4.818484
374.495951	8000.438237	11.628199	-0.074250	4.818497
374.622033	8000.392654	11.633203	-0.074273	4.818483
374.498898	8000.375241	11.638208	-0.074250	4.818478
374.661545	8000.399481	11.643213	-0.074280	4.818485
374.417273	8000.365734	11.648218	-0.074235	4.818476
374.374083	8000.344142	11.653223	-0.074227	4.818469
374.371977	8000.433401	11.658227	-0.074226	4.818496
374.307399	8000.407319	11.663232	-0.074214	4.818488
374.281724	8000.448991	11.668237	-0.074209	4.818501
374.330056	8000.431778	11.673242	-0.074218	4.818496
374.292796	8000.444931	11.678247	-0.074211	4.818500
374.248581	8000.431728	11.683251	-0.074203	4.818496
374.116726	8000.480378	11.688256	-0.074178	4.818511
374.481626	8000.384426	11.693261	-0.074246	4.818481
374.601756	8000.415449	11.698266	-0.074269	4.818490
374.609414	8000.454417	11.703271	-0.074270	4.818501
374.199266	8000.477271	11.708275	-0.074194	4.818510
374.333656	8000.475920	11.713280	-0.074219	4.818509
374.706103	8000.424190	11.718285	-0.074288	4.818492
374.516457	8000.412186	11.723290	-0.074253	4.818489
374.668464	8000.429981	11.728295	-0.074281	4.818494
374.391294	8000.416802	11.733299	-0.074229	4.818491
374.477274	8000.444215	11.738304	-0.074245	4.818499
374.701687	8000.418862	11.743309	-0.074287	4.818490
374.233983	8000.433589	11.748314	-0.074200	4.818497
374.560866	8000.323471	11.753319	-0.074260	4.818462
374.576432	8000.416119	11.758323	-0.074263	4.818490
374.226324	8000.448183	11.763328	-0.074198	4.818501
374.436608	8000.455205	11.768333	-0.074237	4.818502
374.208389	8000.453188	11.773338	-0.074195	4.818502
373.905910	8000.462781	11.778343	-0.074138	4.818507
374.064454	8000.454401	11.783347	-0.074168	4.818503
374.130392	8000.406961	11.788352	-0.074180	4.818489
374.259318	8000.462262	11.793357	-0.074204	4.818505
374.346111	8000.391991	11.798362	-0.074220	4.818484
373.818680	8000.390162	11.803367	-0.074122	4.818485
374.181963	8000.471719	11.808371	-0.074190	4.818508
374.448579	8000.432224	11.813376	-0.074239	4.818495
374.127402	8000.372235	11.818381	-0.074179	4.818479
374.214124	8000.426970	11.823386	-0.074195	4.818495
374.142045	8000.440706	11.828391	-0.074182	4.818499
373.965993	8000.451996	11.833395	-0.074149	4.818503
374.432895	8000.449855	11.838400	-0.074236	4.818501
374.160000	8000.465098	11.843405	-0.074185	4.818506
373.571666	8000.468753	11.848410	-0.074076	4.818510
373.626059	8000.433764	11.853415	-0.074086	4.818499
373.810360	8000.401568	11.858419	-0.074120	4.818489
373.690566	8000.439875	11.863424	-0.074097	4.818501
373.742395	8000.448971	11.868429	-0.074107	4.818503
373.525223	8000.419792	11.873434	-0.074067	4.818495
373.756566	8000.382975	11.878439	-0.074110	4.818483
374.038249	8000.402509	11.883443	-0.074162	4.818488
373.962853	8000.472926	11.888448	-0.074148	4.818509
374.616273	8000.444927	11.893453	-0.074270	4.818498
374.122393	8000.438294	11.898458	-0.074178	4.818498
374.388449	8000.424003	11.903463	-0.074227	4.818493
374.296011	8000.438517	11.908467	-0.074210	4.818498
373.880701	8000.439242	11.913472	-0.074132	4.818500
373.751029	8000.388126	11.918477	-0.074108	4.818485
373.877098	8000.488559	11.923482	-0.074132	4.818514
374.625937	8000.429276	11.928487	-0.074271	4.818494
374.774723	8000.409210	11.933491	-0.074299	4.818487
374.727177	8000.329781	11.938496	-0.074290	4.818464
374.486539	8000.463111	11.943501	-0.074245	4.818504
374.545275	8000.392463	11.948506	-0.074256	4.818483
374.540776	8000.401854	11.953511	-0.074255	4.818486
374.164704	8000.441973	11.958515	-0.074185	4.818499
374.300852	8000.432242	11.963520	-0.074210	4.818496
374.156552	8000.398787	11.968525	-0.074183	4.818487
374.468421	8000.416626	11.973530	-0.074241	4.818491
374.605642	8000.437374	11.978535	-0.074267	4.818496
374.157273	8000.474421	11.983539	-0.074183	4.818509
373.841991	8000.481742	11.988544	-0.074125	4.818512
373.685563	8000.357784	11.993549	-0.074095	4.818476
373.631245	8000.424282	11.998554	-0.074085	4.818496
373.339459	8000.327923	12.003559	-0.074031	4.818469
373.606394	8000.316795	12.008563	-0.074080	4.818464
373.781363	8000.488264	12.013568	-0.074113	4.818515
374.009626	8000.493426	12.018573	-0.074155	4.818515
373.752237	8000.404880	12.023578	-0.074107	4.818490
373.684623	8000.317831	12.028583	-0.074095	4.818464
373.932991	8000.394693	12.033587	-0.074141	4.818486
373.855338	8000.458777	12.038592	-0.074127	4.818506
373.748550	8000.456290	12.043597	-0.074107	4.818505
373.986626	8000.412210	12.048602	-0.074151	4.818491
374.209605	8000.429906	12.053607	-0.074192	4.818496
373.637259	8000.341336	12.058611	-0.074086	4.818472
373.530140	8000.366157	12.063616	-0.074066	4.818479
373.438812	8000.355474	12.068621	-0.074049	4.818477
373.781245	8000.473516	12.073626	-0.074112	4.818510
374.412912	8000.358034	12.078631	-0.074230	4.818473
374.079219	8000.460701	12.083635	-0.074168	4.818505
373.694290	8000.411412	12.088640	-0.074096	4.818492
373.986004	8000.506715	12.093645	-0.074150	4.818519
374.220400	8000.405860	12.098650	-0.074194	4.818488
373.697279	8000.310597	12.103655	-0.074096	4.818462
374.025258	8000.373821	12.108659	-0.074157	4.818480
374.079953	8000.424974	12.113664	-0.074168	4.818495
373.865206	8000.406332	12.118669	-0.074128	4.818490
374.416717	8000.340197	12.123674	-0.074230	4.818468
374.585127	8000.469563	12.128679	-0.074262	4.818506
374.082093	8000.398728	12.133683	-0.074168	4.818487
373.974668	8000.510734	12.138688	-0.074148	4.818521
374.557799	8000.385147	12.143693	-0.074256	4.818481
374.484755	8000.472404	12.148698	-0.074243	4.818507
374.749554	8000.465451	12.153703	-0.074292	4.818504
374.631542	8000.451257	12.158707	-0.074270	4.818500
375.038190	8000.381078	12.163712	-0.074346	4.818478
375.059830	8000.414981	12.168717	-0.074350	4.818488
374.159135	8000.448057	12.173722	-0.074182	4.818501
374.798690	8000.429326	12.178727	-0.074301	4.818493
374.812707	8000.417956	12.183731	-0.074303	4.818490
375.094629	8000.361859	12.188736	-0.074356	4.818472
375.555538	8000.402712	12.193741	-0.074442	4.818482
375.378476	8000.365664	12.198746	-0.074409	4.818472
375.376801	8000.399254	12.203751	-0.074408	4.818482
375.400694	8000.380663	12.208755	-0.074413	4.818476
375.433345	8000.412613	12.213760	-0.074419	4.818486
375.430571	8000.423078	12.218765	-0.074418	4.818489
375.217238	8000.382391	12.223770	-0.074378	4.818477
375.122464	8000.397923	12.228775	-0.074361	4.818482
374.839925	8000.406732	12.233779	-0.074308	4.818486
375.039457	8000.416761	12.238784	-0.074345	4.818488
374.873052	8000.418726	12.243789	-0.074314	4.818490
374.210183	8000.422430	12.248794	-0.074191	4.818493
374.319912	8000.505837	12.253799	-0.074211	4.818518
374.218584	8000.425687	12.258803	-0.074192	4.818494
374.431636	8000.480018	12.263808	-0.074232	4.818510
374.437418	8000.254238	12.268813	-0.074233	4.818443
374.443057	8000.488568	12.273818	-0.074234	4.818512
374.205073	8000.349858	12.278823	-0.074189	4.818472
374.323962	8000.533184	12.283827	-0.074212	4.818526
374.561989	8000.375651	12.288832	-0.074256	4.818478
374.799802	8000.489143	12.293837	-0.074300	4.818511
374.740305	8000.448421	12.298842	-0.074289	4.818499
374.792422	8000.464875	12.303847	-0.074299	4.818504
374.662242	8000.364378	12.308851	-0.074274	4.818474
374.504681	8000.489369	12.313856	-0.074245	4.818512
374.629486	8000.479485	12.318861	-0.074268	4.818509
374.492864	8000.363145	12.323866	-0.074243	4.818475
374.827741	8000.424363	12.328871	-0.074305	4.818492
375.070060	8000.432866	12.333875	-0.074350	4.818493
374.221922	8000.517071	12.338880	-0.074192	4.818522
374.814333	8000.374800	12.343885	-0.074302	4.818477
374.619523	8000.423655	12.348890	-0.074266	4.818492
374.666473	8000.449494	12.353895	-0.074275	4.818500
374.758616	8000.415011	12.358899	-0.074292	4.818489
375.114303	8000.391420	12.363904	-0.074358	4.818481
374.943809	8000.476319	12.368909	-0.074326	4.818507
374.746652	8000.462113	12.373914	-0.074289	4.818503
375.121138	8000.449279	12.378919	-0.074359	4.818498
374.852960	8000.426766	12.383923	-0.074309	4.818492
374.618646	8000.451980	12.388928	-0.074265	4.818501
374.659779	8000.463034	12.393933	-0.074273	4.818504
374.947546	8000.405965	12.398938	-0.074327	4.818486
374.877658	8000.385064	12.403943	-0.074313	4.818480
375.059499	8000.456836	12.408947	-0.074347	4.818500
374.825287	8000.423223	12.413952	-0.074304	4.818491
375.086879	8000.426732	12.418957	-0.074352	4.818491
374.981134	8000.403248	12.423962	-0.074333	4.818485
374.854267	8000.441460	12.428967	-0.074309	4.818497
374.468999	8000.474102	12.433971	-0.074237	4.818508
374.527045	8000.443363	12.438976	-0.074248	4.818498
374.688437	8000.429769	12.443981	-0.074278	4.818494
375.099448	8000.415325	12.448986	-0.074354	4.818488
374.887299	8000.462897	12.453991	-0.074315	4.818503
374.754022	8000.461104	12.458995	-0.074290	4.818503
374.717861	8000.437504	12.464000	-0.074283	4.818496
374.518578	8000.424321	12.469005	-0.074246	4.818493
374.656816	8000.438779	12.474010	-0.074272	4.818497
374.851488	8000.415127	12.479015	-0.074308	4.818489
374.803919	8000.439697	12.484019	-0.074299	4.818496
374.890410	8000.395683	12.489024	-0.074315	4.818483
375.195449	8000.411331	12.494029	-0.074372	4.818486
375.150674	8000.408626	12.499034	-0.074363	4.818486
375.454069	8000.407444	12.504039	-0.074420	4.818484
375.321762	8000.405664	12.509043	-0.074395	4.818484
375.535812	8000.331848	12.514048	-0.074435	4.818461
375.270387	8000.406018	12.519053	-0.074386	4.818484
374.819135	8000.420965	12.524058	-0.074301	4.818491
375.369432	8000.380028	12.529063	-0.074404	4.818476
375.330455	8000.404713	12.534067	-0.074397	4.818484
375.258222	8000.350164	12.539072	-0.074383	4.818468
375.097158	8000.420483	12.544077	-0.074353	4.818489
375.251504	8000.376330	12.549082	-0.074382	4.818476
375.102664	8000.397439	12.554087	-0.074354	4.818482
374.608760	8000.420218	12.559091	-0.074262	4.818491
374.882445	8000.329345	12.564096	-0.074313	4.818463
374.915448	8000.432733	12.569101	-0.074319	4.818494
375.188366	8000.389122	12.574106	-0.074370	4.818480
374.986623	8000.420026	12.579111	-0.074332	4.818490
375.235589	8000.438073	12.584115	-0.074378	4.818494
374.928977	8000.416094	12.589120	-0.074321	4.818489
375.393154	8000.413919	12.594125	-0.074408	4.818486
375.447113	8000.375772	12.599130	-0.074418	4.818475
375.452755	8000.414713	12.604135	-0.074419	4.818486
375.535894	8000.437887	12.609139	-0.074434	4.818493
375.492479	8000.405785	12.614144	-0.074426	4.818483
375.748442	8000.408169	12.619149	-0.074474	4.818483
375.234645	8000.396013	12.624154	-0.074378	4.818482
375.221922	8000.427354	12.629159	-0.074375	4.818491
375.180434	8000.458309	12.634163	-0.074368	4.818500
375.115753	8000.394406	12.639168	-0.074356	4.818482
375.144513	8000.459920	12.644173	-0.074361	4.818501
375.033259	8000.438464	12.649178	-0.074340	4.818495
375.306143	8000.449478	12.654183	-0.074391	4.818497
374.900407	8000.356835	12.659187	-0.074315	4.818471
374.982333	8000.427265	12.664192	-0.074331	4.818492
375.421218	8000.465721	12.669197	-0.074412	4.818502
375.140320	8000.454591	12.674202	-0.074360	4.818499
375.182493	8000.453053	12.679207	-0.074368	4.818499
374.930648	8000.389790	12.684211	-0.074321	4.818481
375.310479	8000.391735	12.689216	-0.074391	4.818480
375.477320	8000.452801	12.694221	-0.074422	4.818497
375.261937	8000.436248	12.699226	-0.074382	4.818493
375.234606	8000.464242	12.704231	-0.074377	4.818502
375.197691	8000.476349	12.709235	-0.074370	4.818506
375.352936	8000.452167	12.714240	-0.074399	4.818498
375.609454	8000.453508	12.719245	-0.074447	4.818497
375.243840	8000.409726	12.724250	-0.074379	4.818486
375.115020	8000.392235	12.729255	-0.074355	4.818481
374.845477	8000.445340	12.734259	-0.074304	4.818498
375.172580	8000.437122	12.739264	-0.074365	4.818494
374.921675	8000.449507	12.744269	-0.074319	4.818499
374.990238	8000.430465	12.749274	-0.074331	4.818493
375.138786	8000.478679	12.754279	-0.074359	4.818507
375.268777	8000.461512	12.759283	-0.074383	4.818501
374.762637	8000.394834	12.764288	-0.074289	4.818483
374.878754	8000.472025	12.769293	-0.074310	4.818506
375.222795	8000.452480	12.774298	-0.074374	4.818498
375.116891	8000.459459	12.779303	-0.074355	4.818501
374.940318	8000.454983	12.784307	-0.074322	4.818500
374.739224	8000.390301	12.789312	-0.074284	4.818482
375.311077	8000.470461	12.794317	-0.074391	4.818503
375.130970	8000.450180	12.799322	-0.074357	4.818498
375.229896	8000.431545	12.804327	-0.074375	4.818492
375.206995	8000.429134	12.809331	-0.074371	4.818492
374.949084	8000.437222	12.814336	-0.074323	4.818495
375.148993	8000.429398	12.819341	-0.074360	4.818492
375.250419	8000.415000	12.824346	-0.074379	4.818487
375.012355	8000.381335	12.829351	-0.074335	4.818478
374.977399	8000.484862	12.834355	-0.074328	4.818509
374.880742	8000.477258	12.839360	-0.074310	4.818507
375.095148	8000.399245	12.844365	-0.074350	4.818483
374.649711	8000.406917	12.849370	-0.074267	4.818487
374.846011	8000.434761	12.854375	-0.074303	4.818495
375.310819	8000.469363	12.859379	-0.074390	4.818503
374.689088	8000.486223	12.864384	-0.074274	4.818511
374.560608	8000.401506	12.869389	-0.074250	4.818486
374.989364	8000.407259	12.874394	-0.074330	4.818486
374.647694	8000.423678	12.879399	-0.074266	4.818492
374.769589	8000.496745	12.884403	-0.074289	4.818513
374.542488	8000.407552	12.889408	-0.074247	4.818488
375.479060	8000.491559	12.894413	-0.074421	4.818509
375.464827	8000.437788	12.899418	-0.074418	4.818493
375.554417	8000.436887	12.904423	-0.074435	4.818492
375.972387	8000.433044	12.909427	-0.074513	4.818490
375.430350	8000.435214	12.914432	-0.074412	4.818492
375.769960	8000.364135	12.919437	-0.074475	4.818470
375.206496	8000.470019	12.924442	-0.074370	4.818504
375.371781	8000.481691	12.929447	-0.074401	4.818507
375.240344	8000.395881	12.934451	-0.074376	4.818482
375.457557	8000.436613	12.939456	-0.074416	4.818493
375.688439	8000.449166	12.944461	-0.074459	4.818496
375.226567	8000.474474	12.949466	-0.074373	4.818505
375.151089	8000.426184	12.954471	-0.074359	4.818491
375.501419	8000.496018	12.959475	-0.074425	4.818510
375.047873	8000.395378	12.964480	-0.074340	4.818482
375.256403	8000.424437	12.969485	-0.074379	4.818490
375.173838	8000.454840	12.974490	-0.074363	4.818499
375.370874	8000.474291	12.979495	-0.074400	4.818504
375.568973	8000.489555	12.984499	-0.074437	4.818508
375.836654	8000.437470	12.989504	-0.074487	4.818492
375.943143	8000.406331	12.994509	-0.074506	4.818482
375.625384	8000.432524	12.999514	-0.074447	4.818491
375.773822	8000.459727	13.004519	-0.074475	4.818498
375.769655	8000.456516	13.009523	-0.074474	4.818497
375.739062	8000.428788	13.014528	-0.074468	4.818489
375.573820	8000.472788	13.019533	-0.074437	4.818503
375.422195	8000.473900	13.024538	-0.074409	4.818504
374.985503	8000.400800	13.029543	-0.074328	4.818484
375.380143	8000.468076	13.034547	-0.074401	4.818502
375.870920	8000.433694	13.039552	-0.074493	4.818490
376.046235	8000.461259	13.044557	-0.074525	4.818498
375.311130	8000.414613	13.049562	-0.074388	4.818487
375.691316	8000.464888	13.054567	-0.074459	4.818500
375.826985	8000.457253	13.059571	-0.074484	4.818497
375.711786	8000.410530	13.064576	-0.074463	4.818484
375.698929	8000.464981	13.069581	-0.074460	4.818500
375.695904	8000.457583	13.074586	-0.074460	4.818498
375.479513	8000.474633	13.079591	-0.074419	4.818504
375.273248	8000.427738	13.084595	-0.074381	4.818491
375.302179	8000.474345	13.089600	-0.074386	4.818505
375.284986	8000.413181	13.094605	-0.074383	4.818487
375.260794	8000.472732	13.099610	-0.074378	4.818504
375.163257	8000.409439	13.104615	-0.074360	4.818486
375.318236	8000.491356	13.109619	-0.074389	4.818510
375.357009	8000.465610	13.114624	-0.074396	4.818502
375.442873	8000.443649	13.119629	-0.074412	4.818495
375.463759	8000.438673	13.124634	-0.074416	4.818493
375.065095	8000.383943	13.129639	-0.074342	4.818479
375.497478	8000.461180	13.134643	-0.074422	4.818500
375.052910	8000.422641	13.139648	-0.074339	4.818490
375.531285	8000.451123	13.144653	-0.074428	4.818497
375.395472	8000.462952	13.149658	-0.074403	4.818501
375.259164	8000.459017	13.154663	-0.074378	4.818500
375.570971	8000.449545	13.159667	-0.074436	4.818496
375.813218	8000.388713	13.164672	-0.074481	4.818477
375.776548	8000.435491	13.169677	-0.074474	4.818491
375.684229	8000.431096	13.174682	-0.074457	4.818490
375.503743	8000.451780	13.179687	-0.074423	4.818497
375.420093	8000.425441	13.184691	-0.074407	4.818490
375.181378	8000.443242	13.189696	-0.074363	4.818496
375.405531	8000.454653	13.194701	-0.074404	4.818498
375.281006	8000.475038	13.199706	-0.074381	4.818505
375.271315	8000.463348	13.204711	-0.074379	4.818502
375.546781	8000.470196	13.209715	-0.074431	4.818502
375.534302	8000.454268	13.214720	-0.074428	4.818498
375.560048	8000.445156	13.219725	-0.074433	4.818495
375.832494	8000.386831	13.224730	-0.074484	4.818477
375.727106	8000.448443	13.229735	-0.074464	4.818495
376.049029	8000.438057	13.234739	-0.074524	4.818491
375.612952	8000.451105	13.239744	-0.074443	4.818497
375.666607	8000.387741	13.244749	-0.074453	4.818477
375.997278	8000.460463	13.249754	-0.074514	4.818498
375.690472	8000.463692	13.254759	-0.074457	4.818500
375.688854	8000.398535	13.259763	-0.074457	4.818481
375.369688	8000.475134	13.264768	-0.074397	4.818505
375.711584	8000.454511	13.269773	-0.074461	4.818497
375.611434	8000.434253	13.274778	-0.074442	4.818492
376.015681	8000.443882	13.279783	-0.074517	4.818493
375.558498	8000.469253	13.284787	-0.074432	4.818502
375.464526	8000.442775	13.289792	-0.074415	4.818495
375.825426	8000.471781	13.294797	-0.074482	4.818502
375.920449	8000.407922	13.299802	-0.074499	4.818482
375.857313	8000.403919	13.304807	-0.074488	4.818482
375.560924	8000.425147	13.309811	-0.074432	4.818489
375.427230	8000.512642	13.314816	-0.074407	4.818516
375.114680	8000.352966	13.319821	-0.074349	4.818469
375.054904	8000.511836	13.324826	-0.074338	4.818517
375.303330	8000.392260	13.329831	-0.074384	4.818480
375.449916	8000.491923	13.334835	-0.074411	4.818509
375.512643	8000.448640	13.339840	-0.074423	4.818496
374.895139	8000.320588	13.344845	-0.074308	4.818461
375.111967	8000.426444	13.349850	-0.074348	4.818491
374.921306	8000.345094	13.354855	-0.074313	4.818468
375.173154	8000.423057	13.359859	-0.074360	4.818490
375.449217	8000.408903	13.364864	-0.074411	4.818485
375.780499	8000.501593	13.369869	-0.074473	4.818511
376.011732	8000.436412	13.374874	-0.074516	4.818491
375.557656	8000.472329	13.379879	-0.074431	4.818503
375.285369	8000.403537	13.384883	-0.074380	4.818484
375.383878	8000.481544	13.389888	-0.074399	4.818507
376.036120	8000.460888	13.394893	-0.074520	4.818498
376.078414	8000.424684	13.399898	-0.074528	4.818487
375.910075	8000.432925	13.404903	-0.074496	4.818490
375.469712	8000.487936	13.409907	-0.074414	4.818508
376.001233	8000.452002	13.414912	-0.074513	4.818495
376.144800	8000.403502	13.419917	-0.074540	4.818480
375.960221	8000.448292	13.424922	-0.074506	4.818494
375.989036	8000.430817	13.429927	-0.074511	4.818489
376.241818	8000.488838	13.434931	-0.074558	4.818505
376.081053	8000.421541	13.439936	-0.074528	4.818486
375.950994	8000.458660	13.444941	-0.074504	4.818497
375.844274	8000.466678	13.449946	-0.074484	4.818500
375.419771	8000.391639	13.454951	-0.074405	4.818480
375.139997	8000.456161	13.459955	-0.074353	4.818500
375.294632	8000.486598	13.464960	-0.074381	4.818508
375.748353	8000.477982	13.469965	-0.074466	4.818504
375.525498	8000.373085	13.474970	-0.074424	4.818474
376.030086	8000.419779	13.479975	-0.074518	4.818486
376.269542	8000.422993	13.484979	-0.074563	4.818486
376.156197	8000.415164	13.489984	-0.074541	4.818484
376.106483	8000.438654	13.494989	-0.074532	4.818491
376.456546	8000.375070	13.499994	-0.074597	4.818471
376.464173	8000.385674	13.504999	-0.074599	4.818474
375.943954	8000.441714	13.510003	-0.074502	4.818492
375.968249	8000.443087	13.515008	-0.074506	4.818493
376.470775	8000.435128	13.520013	-0.074600	4.818488
376.526396	8000.401204	13.525018	-0.074610	4.818478
376.155216	8000.390961	13.530023	-0.074541	4.818477
376.639278	8000.403765	13.535027	-0.074631	4.818478
376.398977	8000.313339	13.540032	-0.074586	4.818453
376.355385	8000.384186	13.545037	-0.074578	4.818474
376.310136	8000.411939	13.550042	-0.074570	4.818482
375.993029	8000.439191	13.555047	-0.074510	4.818492
376.313500	8000.424584	13.560051	-0.074570	4.818486
376.354293	8000.383107	13.565056	-0.074578	4.818473
376.341893	8000.434413	13.570061	-0.074575	4.818489
376.435093	8000.427258	13.575066	-0.074593	4.818486
376.346437	8000.423962	13.580071	-0.074576	4.818486
376.156163	8000.471828	13.585075	-0.074541	4.818501
375.960626	8000.458692	13.590080	-0.074504	4.818497
375.936247	8000.459412	13.595085	-0.074500	4.818498
375.828234	8000.432745	13.600090	-0.074479	4.818490
376.024300	8000.490003	13.605095	-0.074516	4.818507
375.853480	8000.383703	13.610099	-0.074484	4.818476
375.851049	8000.430940	13.615104	-0.074483	4.818490
376.365829	8000.439954	13.620109	-0.074579	4.818490
376.165768	8000.432010	13.625114	-0.074542	4.818489
376.197994	8000.383065	13.630119	-0.074548	4.818474
376.292188	8000.399034	13.635123	-0.074565	4.818478
375.889559	8000.436693	13.640128	-0.074490	4.818491
375.832497	8000.493702	13.645133	-0.074480	4.818508
375.891009	8000.427251	13.650138	-0.074491	4.818488
376.122856	8000.418807	13.655143	-0.074534	4.818485
376.009992	8000.438298	13.660147	-0.074513	4.818491
375.738974	8000.366370	13.665152	-0.074462	4.818471
376.165203	8000.480297	13.670157	-0.074541	4.818503
375.996566	8000.461219	13.675162	-0.074510	4.818498
375.836284	8000.450658	13.680167	-0.074480	4.818496
375.885235	8000.466020	13.685171	-0.074489	4.818500
375.844643	8000.458117	13.690176	-0.074482	4.818498
375.716493	8000.383907	13.695181	-0.074458	4.818476
375.547060	8000.495084	13.700186	-0.074426	4.818510
375.270387	8000.294920	13.705191	-0.074374	4.818452
375.547508	8000.502436	13.710195	-0.074426	4.818512
375.239274	8000.412151	13.715200	-0.074369	4.818487
375.180062	8000.439717	13.720205	-0.074358	4.818495
375.556301	8000.450019	13.725210	-0.074428	4.818497
375.619714	8000.480282	13.730215	-0.074439	4.818505
375.734599	8000.490226	13.735219	-0.074461	4.818508
375.543118	8000.403609	13.740224	-0.074425	4.818483
375.293705	8000.446478	13.745229	-0.074378	4.818497
375.393320	8000.433106	13.750234	-0.074397	4.818492
375.534965	8000.409792	13.755239	-0.074423	4.818485
375.557270	8000.411139	13.760243	-0.074427	4.818485
375.123143	8000.428417	13.765248	-0.074347	4.818492
375.302022	8000.403503	13.770253	-0.074380	4.818484
375.567098	8000.399705	13.775258	-0.074429	4.818482
375.642593	8000.391261	13.780263	-0.074443	4.818479
375.453159	8000.423381	13.785267	-0.074408	4.818489
375.715420	8000.467870	13.790272	-0.074457	4.818501
375.919839	8000.413885	13.795277	-0.074495	4.818484
375.724159	8000.494244	13.800282	-0.074458	4.818509
376.025553	8000.391136	13.805287	-0.074514	4.818477
375.859171	8000.513910	13.810291	-0.074483	4.818514
375.908281	8000.379049	13.815296	-0.074492	4.818474
376.102284	8000.486704	13.820301	-0.074528	4.818505
376.032054	8000.443736	13.825306	-0.074515	4.818493
376.183308	8000.452068	13.830311	-0.074543	4.818495
376.109168	8000.485736	13.835315	-0.074530	4.818505
376.352175	8000.439623	13.840320	-0.074575	4.818490
376.561049	8000.460285	13.845325	-0.074614	4.818496
376.152933	8000.366554	13.850330	-0.074537	4.818469
375.987773	8000.454677	13.855335	-0.074507	4.818496
375.863080	8000.433038	13.860339	-0.074483	4.818490
375.626019	8000.509690	13.865344	-0.074439	4.818514
376.143621	8000.408436	13.870349	-0.074536	4.818482
375.923030	8000.465349	13.875354	-0.074494	4.818500
375.782793	8000.476068	13.880359	-0.074468	4.818503
375.940207	8000.423552	13.885363	-0.074498	4.818487
375.602545	8000.492550	13.890368	-0.074435	4.818509
375.607017	8000.379151	13.895373	-0.074435	4.818475
375.485184	8000.431087	13.900378	-0.074413	4.818491
375.448712	8000.406432	13.905383	-0.074406	4.818484
375.714541	8000.412100	13.910387	-0.074455	4.818485
375.616569	8000.510580	13.915392	-0.074437	4.818514
375.908610	8000.407347	13.920397	-0.074491	4.818482
375.678182	8000.430511	13.925402	-0.074448	4.818490
375.357314	8000.416744	13.930407	-0.074389	4.818487
375.521762	8000.443111	13.935411	-0.074419	4.818495
375.707357	8000.400428	13.940416	-0.074454	4.818481
375.695877	8000.435988	13.945421	-0.074452	4.818492
375.093641	8000.414240	13.950426	-0.074339	4.818488
375.907685	8000.363189	13.955431	-0.074491	4.818469
376.007185	8000.494787	13.960435	-0.074509	4.818508
375.880382	8000.417442	13.965440	-0.074486	4.818486
375.575380	8000.414393	13.970445	-0.074429	4.818486
375.425504	8000.506923	13.975450	-0.074401	4.818514
375.683801	8000.486227	13.980455	-0.074449	4.818507
375.537960	8000.339294	13.985459	-0.074422	4.818464
375.563470	8000.502463	13.990464	-0.074426	4.818512
375.488524	8000.332320	13.995469	-0.074412	4.818462
375.695618	8000.389725	14.000474	-0.074451	4.818478
375.216403	8000.414801	14.005479	-0.074362	4.818487
375.075358	8000.184947	14.010483	-0.074335	4.818420
375.316706	8000.410889	14.015488	-0.074380	4.818486
375.413458	8000.279821	14.020493	-0.074398	4.818447
375.613710	8000.435881	14.025498	-0.074435	4.818492
375.642137	8000.379532	14.030503	-0.074441	4.818475
375.072509	8000.225861	14.035507	-0.074334	4.818432
375.389825	8000.401349	14.040512	-0.074394	4.818483
375.558271	8000.505508	14.045517	-0.074425	4.818513
375.208293	8000.455632	14.050522	-0.074360	4.818500
375.376851	8000.385407	14.055527	-0.074391	4.818478
375.734778	8000.402817	14.060531	-0.074458	4.818482
375.680718	8000.417845	14.065536	-0.074448	4.818487
376.267293	8000.483501	14.070541	-0.074557	4.818504
376.169724	8000.496894	14.075546	-0.074539	4.818508
375.872321	8000.410954	14.080551	-0.074483	4.818484
376.033656	8000.510817	14.085555	-0.074513	4.818513
375.606524	8000.408428	14.090560	-0.074434	4.818484
375.551901	8000.329953	14.095565	-0.074423	4.818461
375.414075	8000.407937	14.100570	-0.074398	4.818485
375.751218	8000.390401	14.105575	-0.074460	4.818478
375.447847	8000.377919	14.110579	-0.074404	4.818476
375.264890	8000.445843	14.115584	-0.074370	4.818497
375.712370	8000.401425	14.120589	-0.074453	4.818482
376.120225	8000.473083	14.125594	-0.074529	4.818501
375.885887	8000.407951	14.130599	-0.074485	4.818483
375.580019	8000.457416	14.135603	-0.074428	4.818499
375.141187	8000.322307	14.140608	-0.074346	4.818460
375.391330	8000.251077	14.145613	-0.074393	4.818438
375.451058	8000.308602	14.150618	-0.074404	4.818455
375.433899	8000.439682	14.155623	-0.074401	4.818494
375.414581	8000.281843	14.160627	-0.074397	4.818447
375.519040	8000.418758	14.165632	-0.074417	4.818487
375.196871	8000.230591	14.170637	-0.074356	4.818433
375.375197	8000.333829	14.175642	-0.074390	4.818463
375.532047	8000.427327	14.180647	-0.074419	4.818490
375.487543	8000.519171	14.185651	-0.074411	4.818517
375.585115	8000.386012	14.190656	-0.074429	4.818477
375.843289	8000.430447	14.195661	-0.074477	4.818490
375.496405	8000.304976	14.200666	-0.074412	4.818454
375.281894	8000.286335	14.205671	-0.074372	4.818449
375.906512	8000.320981	14.210675	-0.074488	4.818457
375.771474	8000.515611	14.215680	-0.074463	4.818515
375.637781	8000.318416	14.220685	-0.074438	4.818457
375.613674	8000.368513	14.225690	-0.074434	4.818472
375.072899	8000.204725	14.230695	-0.074333	4.818426
375.613407	8000.370604	14.235699	-0.074433	4.818473
375.402765	8000.339409	14.240704	-0.074394	4.818464
375.451243	8000.280177	14.245709	-0.074403	4.818447
375.786175	8000.325641	14.250714	-0.074465	4.818459
375.230147	8000.350737	14.255719	-0.074362	4.818468
375.732027	8000.377433	14.260723	-0.074455	4.818474
375.238272	8000.327729	14.265728	-0.074363	4.818462
375.587459	8000.200050	14.270733	-0.074428	4.818422
376.026902	8000.483285	14.275738	-0.074510	4.818505
375.931753	8000.411618	14.280743	-0.074492	4.818484
375.649399	8000.277559	14.285747	-0.074440	4.818445
375.681170	8000.433458	14.290752	-0.074446	4.818491
375.506806	8000.321860	14.295757	-0.074413	4.818459
375.894508	8000.342820	14.300762	-0.074485	4.818463
375.920762	8000.480788	14.305767	-0.074490	4.818504
375.966304	8000.437274	14.310771	-0.074498	4.818491
375.714170	8000.419177	14.315776	-0.074451	4.818487
375.513975	7999.416429	14.320781	-0.074413	4.818190

375.244829	7996.384684	14.325786	-0.074361	4.817290
375.473180	7990.773020	14.330791	-0.074400	4.815620
375.197428	7984.089345	14.335795	-0.074344	4.813633
375.002589	7976.848357	14.340800	-0.074303	4.811480
374.984095	7969.156834	14.345805	-0.074295	4.809190
375.059249	7961.386321	14.350810	-0.074304	4.806875
375.185770	7953.408578	14.355815	-0.074322	4.804497
375.208228	7945.581103	14.360819	-0.074321	4.802164
375.217926	7937.499862	14.365824	-0.074318	4.799753
375.547096	7929.558211	14.370829	-0.074374	4.797382
375.260096	7921.529640	14.375834	-0.074315	4.794986
374.854636	7913.626107	14.380839	-0.074234	4.792626
374.911671	7905.650320	14.385843	-0.074240	4.790242
374.963126	7897.562568	14.390848	-0.074244	4.787824
374.575381	7889.582674	14.395853	-0.074166	4.785438
374.940786	7881.632588	14.400858	-0.074229	4.783057
374.815778	7873.564522	14.405863	-0.074201	4.780641
374.976555	7865.552455	14.410867	-0.074225	4.778240
375.247275	7857.536088	14.415872	-0.074270	4.775836
374.793144	7849.593586	14.420877	-0.074181	4.773455
374.425274	7841.623810	14.425882	-0.074107	4.771065
374.394304	7833.544907	14.430887	-0.074096	4.768639
374.463041	7825.541707	14.435891	-0.074103	4.766235
374.695279	7817.442222	14.440896	-0.074141	4.763800
374.885575	7809.551955	14.445901	-0.074172	4.761427
374.795428	7801.501293	14.450906	-0.074149	4.759005
374.658743	7793.550819	14.455911	-0.074119	4.756612
374.418290	7785.524783	14.460915	-0.074069	4.754196
374.224962	7777.567534	14.465920	-0.074028	4.751799
373.915554	7769.526502	14.470925	-0.073965	4.749376
373.912101	7761.519980	14.475930	-0.073959	4.746961
373.799976	7753.483635	14.480935	-0.073933	4.744536
374.381529	7745.552621	14.485939	-0.074036	4.742140
373.836804	7737.490363	14.490944	-0.073929	4.739706
374.072556	7729.524568	14.495949	-0.073968	4.737298
373.694170	7721.527682	14.500954	-0.073892	4.734881
373.371146	7713.544677	14.505959	-0.073826	4.732466
374.189395	7705.413219	14.510963	-0.073973	4.730003
373.902402	7697.472718	14.515968	-0.073915	4.727599
373.524604	7689.510088	14.520973	-0.073839	4.725187
373.411336	7681.545978	14.525978	-0.073813	4.722772
373.298485	7673.514993	14.530983	-0.073787	4.720337
373.351516	7665.568279	14.535987	-0.073791	4.717925
373.172430	7657.568920	14.540992	-0.073753	4.715496
373.523959	7649.489041	14.545997	-0.073813	4.713041
374.043764	7641.460252	14.551002	-0.073904	4.710600
373.656025	7633.448764	14.556007	-0.073827	4.708164
373.806326	7625.488027	14.561011	-0.073850	4.705742
373.468630	7617.490355	14.566016	-0.073781	4.703308
373.220631	7609.569049	14.571021	-0.073730	4.700895
373.452986	7601.473456	14.576026	-0.073768	4.698428
373.233128	7593.506336	14.581031	-0.073722	4.695999
373.355609	7585.514913	14.586035	-0.073739	4.693561
373.108888	7577.565290	14.591040	-0.073688	4.691135
372.947359	7569.475003	14.596045	-0.073653	4.688665
373.061941	7561.517513	14.601050	-0.073669	4.686233
373.067846	7553.404558	14.606055	-0.073665	4.683753
372.785630	7545.573802	14.611059	-0.073607	4.681358
372.679257	7537.510933	14.616064	-0.073582	4.678891
372.731698	7529.545451	14.621069	-0.073586	4.676452
372.662449	7521.474874	14.626074	-0.073568	4.673980
372.552333	7513.441122	14.631079	-0.073542	4.671517
372.690765	7505.405906	14.636083	-0.073563	4.669053
372.452413	7497.445628	14.641088	-0.073513	4.666611
372.202711	7489.412338	14.646093	-0.073462	4.664145
372.445559	7481.514903	14.651098	-0.073502	4.661719
372.285560	7473.414042	14.656103	-0.073466	4.659229
372.221771	7465.512521	14.661107	-0.073449	4.656800
372.076775	7457.474113	14.666112	-0.073417	4.654327
371.878482	7449.490738	14.671117	-0.073375	4.651870
372.133512	7441.421413	14.676122	-0.073417	4.649384
371.733185	7433.450723	14.681127	-0.073337	4.646928
372.028991	7425.430397	14.686131	-0.073387	4.644456
371.740399	7417.497619	14.691136	-0.073328	4.642009
371.564095	7409.466903	14.696141	-0.073290	4.639530
371.652517	7401.505964	14.701146	-0.073301	4.637072
371.889667	7393.342945	14.706151	-0.073340	4.634550
371.531533	7385.465857	14.711155	-0.073268	4.632115
371.584338	7377.471272	14.716160	-0.073273	4.629642
371.539350	7369.475078	14.721165	-0.073259	4.627168
371.146934	7361.437534	14.726170	-0.073181	4.624679
371.094879	7353.431920	14.731175	-0.073166	4.622199
371.570060	7345.383018	14.736179	-0.073249	4.619704
371.412003	7337.438591	14.741184	-0.073214	4.617240
371.405966	7329.384380	14.746189	-0.073208	4.614741
371.395767	7321.441120	14.751194	-0.073201	4.612275
371.778284	7313.287837	14.756199	-0.073267	4.609743
371.702412	7305.380477	14.761203	-0.073247	4.607285
371.301394	7297.375167	14.766208	-0.073167	4.604795
371.530291	7289.459227	14.771213	-0.073205	4.602333
371.222537	7281.432284	14.776218	-0.073142	4.599834
370.930563	7273.432813	14.781223	-0.073083	4.597342
371.149575	7265.399504	14.786227	-0.073118	4.594838
370.858549	7257.450910	14.791232	-0.073059	4.592360
370.568243	7249.371670	14.796237	-0.072999	4.589839
371.044547	7241.361168	14.801242	-0.073083	4.587339
371.422227	7233.302401	14.806247	-0.073148	4.584822
371.466890	7225.388536	14.811251	-0.073151	4.582349
371.218996	7217.339805	14.816256	-0.073099	4.579833
371.127362	7209.422412	14.821261	-0.073077	4.577356
371.165293	7201.351028	14.826266	-0.073079	4.574829
371.233337	7193.328759	14.831271	-0.073086	4.572317
371.016923	7185.320649	14.836275	-0.073041	4.569807
370.646347	7177.405642	14.841280	-0.072967	4.567325
370.729719	7169.322900	14.846285	-0.072977	4.564789
371.162581	7161.381425	14.851290	-0.073052	4.562298
370.746715	7153.292134	14.856295	-0.072969	4.559756
370.960252	7145.355898	14.861299	-0.073004	4.557263
370.999980	7137.295182	14.866304	-0.073006	4.554729
371.123842	7129.358355	14.871309	-0.073024	4.552233
371.020648	7121.330447	14.876314	-0.072999	4.549706
370.451997	7113.367300	14.881319	-0.072888	4.547197
370.435342	7105.367564	14.886323	-0.072880	4.544676
370.336031	7097.382882	14.891328	-0.072856	4.542158
369.967022	7089.349600	14.896333	-0.072782	4.539623
370.021626	7081.387420	14.901338	-0.072787	4.537110
370.442379	7073.260287	14.906343	-0.072860	4.534545
370.406403	7065.331469	14.911347	-0.072848	4.532040
370.013430	7057.310714	14.916352	-0.072770	4.529503
370.649017	7049.226501	14.921357	-0.072883	4.526947
370.416132	7041.283335	14.926362	-0.072834	4.524433
370.322122	7033.356106	14.931367	-0.072812	4.521922
370.387163	7025.308575	14.936371	-0.072818	4.519372
369.731820	7017.405962	14.941376	-0.072691	4.516865
370.646085	7009.237528	14.946381	-0.072856	4.514276
369.963395	7001.393524	14.951386	-0.072724	4.511784
369.437717	6993.323416	14.956391	-0.072621	4.509220
369.639214	6985.294186	14.961395	-0.072653	4.506669
369.640315	6977.213792	14.966400	-0.072648	4.504100
369.741977	6969.339942	14.971405	-0.072661	4.501595
370.077710	6961.229414	14.976410	-0.072719	4.499015
369.489084	6953.292244	14.981415	-0.072604	4.496485
369.398925	6945.290062	14.986419	-0.072582	4.493935
369.602619	6937.209551	14.991424	-0.072614	4.491359
369.604244	6929.174290	14.996429	-0.072609	4.488796
369.649385	6921.258449	15.001434	-0.072613	4.486269
369.343625	6913.260713	15.006439	-0.072550	4.483713
369.539552	6905.265967	15.011443	-0.072582	4.481159
369.370547	6897.253238	15.016448	-0.072545	4.478596
369.414475	6889.242295	15.021453	-0.072548	4.476033
369.262584	6881.272738	15.026458	-0.072514	4.473481
369.004378	6873.236193	15.031463	-0.072461	4.470906
369.106299	6865.198342	15.036467	-0.072475	4.468330
368.730487	6857.267298	15.041472	-0.072399	4.465785
368.736427	6849.234243	15.046477	-0.072395	4.463208
368.847810	6841.254840	15.051482	-0.072411	4.460647
368.646480	6833.218564	15.056487	-0.072368	4.458064
368.933187	6825.215611	15.061491	-0.072416	4.455493
368.249292	6817.289234	15.066496	-0.072283	4.452941
368.445449	6809.228970	15.071501	-0.072315	4.450348
368.733200	6801.197104	15.076506	-0.072363	4.447763
368.607994	6793.118214	15.081511	-0.072334	4.445160
368.248956	6785.289913	15.086515	-0.072262	4.442634
368.108998	6777.256551	15.091520	-0.072231	4.440042
368.171954	6769.228480	15.096525	-0.072237	4.437452
367.966482	6761.245301	15.101530	-0.072194	4.434873
367.927708	6753.195473	15.106535	-0.072181	4.432271
367.598324	6745.248009	15.111539	-0.072115	4.429700
367.872408	6737.146345	15.116544	-0.072161	4.427081
367.883663	6729.159045	15.121549	-0.072157	4.424495
367.727646	6721.238141	15.126554	-0.072123	4.421929
367.448739	6713.172885	15.131559	-0.072066	4.419314
367.532791	6705.225352	15.136563	-0.072076	4.416737
367.683303	6697.144626	15.141568	-0.072099	4.414116
367.768281	6689.149646	15.146573	-0.072110	4.411521
367.988339	6681.131857	15.151578	-0.072145	4.408918
367.874451	6673.165315	15.156583	-0.072119	4.406328
367.461831	6665.256192	15.161587	-0.072037	4.403753
367.376947	6657.243929	15.166592	-0.072016	4.401146
367.407787	6649.222719	15.171597	-0.072016	4.398534
367.624468	6641.226590	15.176602	-0.072051	4.395930
367.325249	6633.230930	15.181607	-0.071990	4.393322
367.278853	6625.262860	15.186611	-0.071977	4.390723
367.089166	6617.245997	15.191616	-0.071936	4.388105
367.178233	6609.205408	15.196621	-0.071947	4.385479
367.398089	6601.200355	15.201626	-0.071983	4.382865
367.253685	6593.179851	15.206631	-0.071951	4.380242
367.358206	6585.215306	15.211635	-0.071965	4.377637
367.521710	6577.195114	15.216640	-0.071990	4.375012
366.943299	6569.265962	15.221645	-0.071877	4.372411
367.192625	6561.239256	15.226650	-0.071918	4.369782
367.160075	6553.222440	15.231655	-0.071907	4.367153
367.326408	6545.209933	15.236659	-0.071933	4.364525
367.374667	6537.294148	15.241664	-0.071937	4.361926
367.279563	6529.215260	15.246669	-0.071913	4.359271
367.533882	6521.281610	15.251674	-0.071956	4.356665
367.321907	6513.195218	15.256679	-0.071911	4.354003
367.808287	6505.180430	15.261683	-0.071996	4.351369
367.535698	6497.211461	15.266688	-0.071940	4.348742
367.322916	6489.191104	15.271693	-0.071895	4.346098
367.156383	6481.257935	15.276698	-0.071859	4.343480
366.958711	6473.224410	15.281703	-0.071817	4.340828
366.746255	6465.275645	15.286707	-0.071772	4.338202
366.736258	6457.244736	15.291712	-0.071765	4.335549
366.605229	6449.272667	15.296717	-0.071735	4.332913
366.665017	6441.236695	15.301722	-0.071741	4.330256
366.697654	6433.203478	15.306727	-0.071742	4.327597
366.697596	6425.222182	15.311731	-0.071737	4.324954
366.450414	6417.254763	15.316736	-0.071685	4.322312
366.462418	6409.255685	15.321741	-0.071682	4.319660
366.284913	6401.343463	15.326746	-0.071644	4.317033
366.073154	6393.233001	15.331751	-0.071599	4.314339
366.536669	6385.193948	15.336755	-0.071680	4.311672
366.146436	6377.206228	15.341760	-0.071603	4.309014
365.786800	6369.271601	15.346765	-0.071530	4.306372
365.706333	6361.239934	15.351770	-0.071510	4.303698
365.866450	6353.199427	15.356775	-0.071535	4.301022
365.525263	6345.240939	15.361779	-0.071466	4.298367
365.424880	6337.263254	15.366784	-0.071442	4.295706
365.349343	6329.207568	15.371789	-0.071423	4.293018
365.557030	6321.206268	15.376794	-0.071456	4.290349
365.690587	6313.119414	15.381799	-0.071476	4.287648
365.806176	6305.158553	15.386803	-0.071492	4.284988
365.403659	6297.237557	15.391808	-0.071412	4.282335
365.677606	6289.152526	15.396813	-0.071457	4.279632
365.486033	6281.262720	15.401818	-0.071417	4.276988
365.240505	6273.181962	15.406823	-0.071365	4.274278
365.385351	6265.207883	15.411827	-0.071387	4.271605
365.410568	6257.161266	15.416832	-0.071387	4.268906
365.621333	6249.133873	15.421837	-0.071421	4.266213
365.654083	6241.210503	15.426842	-0.071421	4.263551
365.330721	6233.196704	15.431847	-0.071356	4.260854
365.209028	6225.222047	15.436851	-0.071328	4.258170
364.690839	6217.250379	15.441856	-0.071226	4.255482
364.829982	6209.214215	15.446861	-0.071247	4.252777
365.046649	6201.169664	15.451866	-0.071282	4.250068
364.710042	6193.152520	15.456871	-0.071214	4.247361
365.103434	6185.147912	15.461875	-0.071282	4.244664
365.072215	6177.214912	15.466880	-0.071271	4.241985
365.064419	6169.131959	15.471885	-0.071264	4.239254
364.832593	6161.260598	15.476890	-0.071216	4.236590
364.735283	6153.190806	15.481895	-0.071193	4.233859
364.700228	6145.193449	15.486899	-0.071181	4.231151
364.877115	6137.144757	15.491904	-0.071208	4.228426
365.017164	6129.111571	15.496909	-0.071229	4.225705
365.810250	6121.073580	15.501914	-0.071372	4.222987
365.339985	6113.137360	15.506919	-0.071279	4.220289
365.251970	6105.173774	15.511923	-0.071257	4.217583
365.118249	6097.169998	15.516928	-0.071227	4.214862
365.221766	6089.162734	15.521933	-0.071241	4.212140
364.820996	6081.221320	15.526938	-0.071161	4.209433
365.032348	6073.175904	15.531943	-0.071195	4.206696
365.008218	6065.156353	15.536947	-0.071185	4.203963
365.144555	6057.218102	15.541952	-0.071206	4.201258
364.894530	6049.187305	15.546957	-0.071154	4.198516
365.383234	6041.159565	15.551962	-0.071239	4.195781
364.535142	6033.199093	15.556967	-0.071076	4.193052
364.713687	6025.125716	15.561971	-0.071104	4.190294
365.036841	6017.121011	15.566976	-0.071159	4.187560
365.060275	6009.089905	15.571981	-0.071158	4.184811
364.736742	6001.207441	15.576986	-0.071093	4.182107
364.113584	5993.195976	15.581991	-0.070972	4.179354
364.641947	5985.214800	15.586995	-0.071065	4.176623
364.088737	5977.196204	15.592000	-0.070956	4.173865
364.214157	5969.136131	15.597005	-0.070974	4.171098
364.140276	5961.153926	15.602010	-0.070955	4.168354
363.727971	5953.200153	15.607015	-0.070873	4.165614
363.994536	5945.210765	15.612019	-0.070918	4.162868
363.752753	5937.212510	15.617024	-0.070868	4.160111
363.847052	5929.189191	15.622029	-0.070880	4.157348
363.838102	5921.211199	15.627034	-0.070873	4.154597
363.633119	5913.223171	15.632039	-0.070830	4.151839
363.724888	5905.204149	15.637043	-0.070841	4.149071
363.198541	5897.257919	15.642048	-0.070738	4.146319
363.778584	5889.144533	15.647053	-0.070841	4.143522
363.973851	5881.203457	15.652058	-0.070872	4.140777
363.542814	5873.189573	15.657063	-0.070786	4.137998
363.839062	5865.147985	15.662067	-0.070836	4.135216
363.720613	5857.196992	15.667072	-0.070809	4.132458
363.577064	5849.164158	15.672077	-0.070777	4.129670
363.279752	5841.222822	15.677082	-0.070716	4.126910
363.101602	5833.165462	15.682087	-0.070678	4.124108
363.086845	5825.282332	15.687091	-0.070670	4.121368
363.255314	5817.145975	15.692096	-0.070696	4.118541
363.128741	5809.210673	15.697101	-0.070667	4.115777
363.379653	5801.172516	15.702106	-0.070709	4.112981
363.267388	5793.183830	15.707111	-0.070682	4.110195
363.328678	5785.182888	15.712115	-0.070689	4.107406
363.044548	5777.195077	15.717120	-0.070630	4.104614
363.100484	5769.204365	15.722125	-0.070636	4.101824
362.763605	5761.197608	15.727130	-0.070568	4.099021
363.389273	5753.155195	15.732135	-0.070679	4.096218
363.098749	5745.190587	15.737139	-0.070620	4.093426
362.782562	5737.207649	15.742144	-0.070555	4.090626
362.597121	5729.212408	15.747149	-0.070516	4.087822
363.133400	5721.117805	15.752154	-0.070610	4.084991
362.405505	5713.277356	15.757159	-0.070469	4.082229
362.310850	5705.205167	15.762163	-0.070447	4.079393
362.663546	5697.180956	15.767168	-0.070507	4.076578
362.546171	5689.177727	15.772173	-0.070480	4.073762
362.016684	5681.289956	15.777178	-0.070376	4.070979
362.276336	5673.157642	15.782183	-0.070419	4.068119
362.739100	5665.116058	15.787187	-0.070500	4.065292
362.265033	5657.232904	15.792192	-0.070406	4.062505
362.258510	5649.167841	15.797197	-0.070400	4.059659
362.377675	5641.225797	15.802202	-0.070417	4.056857
361.823118	5633.240197	15.807207	-0.070308	4.054026
361.945772	5625.244645	15.812211	-0.070326	4.051201
361.888303	5617.184118	15.817216	-0.070310	4.048348
361.987639	5609.151408	15.822221	-0.070323	4.045505
361.510641	5601.282189	15.827226	-0.070229	4.042709
361.250005	5593.281289	15.832231	-0.070175	4.039867
361.461251	5585.288596	15.837235	-0.070209	4.037035
362.042559	5577.158114	15.842240	-0.070312	4.034157
361.599981	5569.148277	15.847245	-0.070225	4.031303
361.748598	5561.152399	15.852250	-0.070247	4.028462
361.329965	5553.210058	15.857255	-0.070164	4.025629
361.409695	5545.217227	15.862259	-0.070174	4.022784
361.680790	5537.153738	15.867264	-0.070219	4.019915
361.503374	5529.246255	15.872269	-0.070180	4.017092
361.645743	5521.179078	15.877274	-0.070202	4.014215
361.082408	5513.276530	15.882279	-0.070092	4.011384
361.147829	5505.225353	15.887283	-0.070098	4.008507
360.932804	5497.239430	15.892288	-0.070053	4.005647
360.453142	5489.285812	15.897293	-0.069959	4.002793
361.085918	5481.248502	15.902298	-0.070071	3.999925
360.715524	5473.266406	15.907303	-0.069997	3.997058
361.085947	5465.185025	15.912307	-0.070061	3.994165
360.460747	5457.315588	15.917312	-0.069939	3.991330
361.180047	5449.161038	15.922317	-0.070068	3.988413
360.954665	5441.229969	15.927322	-0.070020	3.985559
360.637438	5433.282269	15.932327	-0.069956	3.982694
360.988581	5425.207989	15.937331	-0.070016	3.979794
360.432832	5417.346055	15.942336	-0.069908	3.976952
360.420280	5409.229423	15.947341	-0.069900	3.974026
360.894783	5401.232190	15.952346	-0.069983	3.971149
361.189173	5393.167396	15.957351	-0.070032	3.968243
361.023549	5385.206522	15.962355	-0.069996	3.965364
360.815256	5377.288174	15.967360	-0.069952	3.962497
361.174660	5369.226318	15.972365	-0.070014	3.959587
360.497863	5361.382919	15.977370	-0.069883	3.956734
360.378539	5353.277751	15.982375	-0.069855	3.953795
360.345961	5345.291301	15.987379	-0.069844	3.950899
360.367224	5337.236595	15.992384	-0.069843	3.947976
360.373498	5329.198073	15.997389	-0.069839	3.945057
359.959638	5321.328835	16.002394	-0.069756	3.942190
360.355581	5313.194528	16.007399	-0.069825	3.939239
360.249515	5305.313429	16.012403	-0.069800	3.936368
360.588064	5297.206763	16.017408	-0.069857	3.933422
360.712922	5289.225085	16.022413	-0.069875	3.930515
360.971579	5281.234546	16.027418	-0.069918	3.927606
360.632197	5273.209500	16.032423	-0.069850	3.924670
360.298956	5265.323557	16.037427	-0.069783	3.921782
360.380485	5257.325959	16.042432	-0.069793	3.918860
360.454876	5249.286909	16.047437	-0.069801	3.915920
360.018697	5241.380027	16.052442	-0.069715	3.913017
360.041228	5233.307256	16.057447	-0.069714	3.910060
359.724077	5225.367813	16.062451	-0.069649	3.907142
359.394250	5217.367091	16.067456	-0.069583	3.904200
359.097039	5209.419219	16.072461	-0.069522	3.901275
359.225617	5201.370211	16.077466	-0.069541	3.898319
358.958278	5193.323419	16.082471	-0.069486	3.895354
358.988598	5185.360680	16.087475	-0.069486	3.892424
359.566153	5177.217104	16.092480	-0.069588	3.889436
359.041666	5169.323215	16.097485	-0.069485	3.886515
359.124915	5161.335856	16.102490	-0.069496	3.883570
359.337386	5153.292403	16.107495	-0.069530	3.880605
359.230483	5145.388538	16.112499	-0.069505	3.877683
359.057026	5137.360210	16.117504	-0.069467	3.874710
358.918627	5129.240857	16.122509	-0.069436	3.871703
359.749530	5121.161750	16.127514	-0.069586	3.868728
359.241015	5113.225701	16.132519	-0.069486	3.865776
359.178611	5105.317750	16.137523	-0.069469	3.862842
359.147195	5097.283759	16.142528	-0.069458	3.859859
359.158499	5089.312366	16.147533	-0.069455	3.856898
358.765414	5081.383702	16.152538	-0.069376	3.853942
358.990525	5073.321737	16.157543	-0.069413	3.850948
359.079364	5065.293930	16.162547	-0.069424	3.847961
359.124078	5057.290793	16.167552	-0.069427	3.844980
358.559035	5049.404583	16.172557	-0.069317	3.842026
359.104662	5041.318642	16.177562	-0.069413	3.839021
358.584242	5033.423127	16.182567	-0.069311	3.836060
358.317187	5025.422226	16.187571	-0.069256	3.833064
358.609091	5017.386462	16.192576	-0.069305	3.830064
358.606790	5009.365077	16.197581	-0.069299	3.827061
358.590108	5001.328358	16.202586	-0.069291	3.824050
358.520299	4993.372719	16.207591	-0.069273	3.821065
358.621140	4985.344130	16.212595	-0.069286	3.818054
358.414993	4977.374272	16.217600	-0.069243	3.815057
358.189170	4969.382065	16.222605	-0.069195	3.812048
358.311609	4961.350412	16.227610	-0.069213	3.809029
358.063143	4953.405515	16.232615	-0.069161	3.806033
358.062836	4945.375743	16.237619	-0.069156	3.803008
357.818716	4937.446646	16.242624	-0.069105	3.800012
357.911633	4929.421484	16.247629	-0.069117	3.796986
358.191418	4921.337538	16.252634	-0.069164	3.793940
358.039440	4913.407848	16.257639	-0.069131	3.790939
358.079086	4905.355555	16.262643	-0.069133	3.787894
358.160742	4897.366485	16.267648	-0.069143	3.784872
358.241122	4889.412678	16.272653	-0.069152	3.781860
357.788543	4881.505707	16.277658	-0.069063	3.778852
357.781409	4873.412988	16.282663	-0.069056	3.775781
357.522612	4865.485581	16.287667	-0.069003	3.772764
357.744472	4857.379301	16.292672	-0.069039	3.769688
358.175779	4849.365636	16.297677	-0.069114	3.766650
357.586973	4841.442313	16.302682	-0.068999	3.763620
357.843162	4833.431185	16.307687	-0.069041	3.760573
357.438389	4825.518339	16.312691	-0.068961	3.757546
357.083034	4817.505870	16.317696	-0.068889	3.754480
357.558923	4809.449451	16.322701	-0.068973	3.751414
357.630200	4801.439224	16.327706	-0.068981	3.748354
357.309809	4793.459873	16.332711	-0.068916	3.745294
357.389152	4785.510323	16.337715	-0.068925	3.742252
357.138071	4777.496548	16.342720	-0.068873	3.739175
357.348750	4769.493714	16.347725	-0.068907	3.736111
357.011223	4761.522451	16.352730	-0.068839	3.733043
356.716942	4753.516081	16.357735	-0.068779	3.729960
357.562553	4745.433753	16.362739	-0.068931	3.726874
357.086697	4737.500448	16.367744	-0.068837	3.723809
357.231512	4729.475496	16.372749	-0.068859	3.720723
357.250127	4721.526206	16.377754	-0.068857	3.717659
357.351040	4713.469606	16.382759	-0.068871	3.714554
356.974612	4705.504755	16.387763	-0.068796	3.711470
356.709592	4697.528779	16.392768	-0.068741	3.708381
356.869943	4689.473861	16.397773	-0.068766	3.705270
356.610881	4681.577106	16.402778	-0.068712	3.702207
356.240147	4673.557549	16.407783	-0.068638	3.699091
356.650291	4665.542215	16.412787	-0.068709	3.695994
356.496220	4657.521681	16.417792	-0.068675	3.692878
356.115496	4649.541835	16.422797	-0.068599	3.689769
356.672247	4641.496346	16.427802	-0.068697	3.686657
356.692816	4633.482722	16.432807	-0.068696	3.683540
356.459570	4625.583000	16.437811	-0.068647	3.680459
356.603956	4617.560805	16.442816	-0.068669	3.677337
356.412967	4609.549212	16.447821	-0.068628	3.674207
356.330265	4601.617024	16.452826	-0.068607	3.671109
356.406938	4593.524784	16.457831	-0.068616	3.667950
356.396060	4585.521381	16.462835	-0.068609	3.664820
356.484071	4577.595308	16.467840	-0.068620	3.661721
356.099217	4569.620424	16.472845	-0.068543	3.658587
355.847339	4561.684656	16.477850	-0.068491	3.655470
356.035442	4553.619943	16.482855	-0.068521	3.652311
355.878778	4545.614175	16.487859	-0.068486	3.649163
355.783257	4537.646814	16.492864	-0.068463	3.646029
355.790036	4529.606133	16.497869	-0.068459	3.642866
355.999557	4521.642095	16.502874	-0.068493	3.639737
355.573923	4513.701437	16.507879	-0.068409	3.636596
355.513103	4505.692783	16.512883	-0.068392	3.633436
355.485038	4497.674559	16.517888	-0.068382	3.630270
355.338175	4489.637891	16.522893	-0.068349	3.627091
355.079269	4481.696890	16.527898	-0.068296	3.623944
354.989343	4473.695542	16.532903	-0.068274	3.620775
355.320777	4465.645605	16.537907	-0.068330	3.617596
355.066826	4457.658371	16.542912	-0.068277	3.614422
355.216613	4449.642668	16.547917	-0.068300	3.611245
355.164725	4441.694211	16.552922	-0.068285	3.608087
354.835811	4433.687391	16.557927	-0.068219	3.604895
354.569235	4425.774242	16.562931	-0.068164	3.601739
355.178949	4417.649469	16.567936	-0.068272	3.598521
355.140364	4409.657687	16.572941	-0.068260	3.595335
354.795299	4401.766809	16.577946	-0.068190	3.592177
354.424299	4393.763021	16.582951	-0.068116	3.588971
355.091098	4385.645874	16.587955	-0.068235	3.585747
354.891023	4377.722669	16.592960	-0.068192	3.582571
354.859126	4369.698950	16.597965	-0.068181	3.579358
354.752560	4361.788501	16.602970	-0.068156	3.576185
354.999989	4353.697536	16.607975	-0.068197	3.572948
354.615403	4345.773219	16.612979	-0.068120	3.569755
354.502897	4337.808496	16.617984	-0.068094	3.566552
354.458086	4329.776811	16.622989	-0.068080	3.563321
354.740127	4321.781963	16.627994	-0.068127	3.560111
354.281186	4313.873677	16.632999	-0.068037	3.556911
353.948792	4305.865583	16.638003	-0.067969	3.553672
354.001158	4297.786890	16.643008	-0.067974	3.550413
354.122407	4289.743544	16.648013	-0.067991	3.547167
354.230664	4281.729342	16.653018	-0.068006	3.543930
353.729508	4273.861016	16.658023	-0.067908	3.540730
353.813901	4265.838594	16.663027	-0.067918	3.537483
354.047087	4257.782765	16.668032	-0.067956	3.534223
354.123154	4249.811023	16.673037	-0.067965	3.530991
354.051241	4241.798120	16.678042	-0.067946	3.527733
354.073762	4233.780700	16.683047	-0.067945	3.524474
354.029752	4225.879401	16.688051	-0.067932	3.521258
353.899697	4217.861075	16.693056	-0.067902	3.517987
353.827605	4209.891648	16.698061	-0.067884	3.514736
354.025854	4201.884680	16.703066	-0.067915	3.511474
354.120482	4193.812250	16.708071	-0.067928	3.508180
354.086670	4185.819332	16.713075	-0.067916	3.504911
354.162517	4177.873249	16.718080	-0.067925	3.501662
353.947591	4169.889028	16.723085	-0.067880	3.498384
353.614878	4161.979610	16.728090	-0.067813	3.495130
353.733267	4153.929958	16.733095	-0.067829	3.491831
353.228121	4145.974185	16.738099	-0.067730	3.488546
353.430990	4137.942073	16.743104	-0.067763	3.485250
353.560458	4129.915786	16.748109	-0.067781	3.481951
353.758950	4121.906641	16.753114	-0.067813	3.478658
353.712654	4113.955028	16.758119	-0.067799	3.475378
353.705547	4105.951827	16.763123	-0.067793	3.472075
353.840565	4097.934148	16.768128	-0.067813	3.468767
353.698279	4089.907366	16.773133	-0.067781	3.465443
353.360947	4082.037695	16.778138	-0.067713	3.462174
353.247176	4074.015000	16.783143	-0.067686	3.458846
353.378067	4066.016166	16.788147	-0.067705	3.455534
353.250531	4058.049167	16.793152	-0.067676	3.452222
352.947557	4050.041227	16.798157	-0.067615	3.448884
352.621701	4042.111348	16.803162	-0.067549	3.445575
352.716703	4034.059260	16.808167	-0.067561	3.442226
352.577832	4026.074784	16.813171	-0.067530	3.438894
352.857935	4018.064815	16.818176	-0.067577	3.435563
352.456989	4010.121428	16.823181	-0.067497	3.432232
352.396515	4002.103777	16.828186	-0.067481	3.428879
353.009952	3993.955589	16.833191	-0.067590	3.425492
352.667070	3986.084617	16.838195	-0.067520	3.422184
352.524079	3978.109336	16.843200	-0.067489	3.418836
352.190808	3970.164658	16.848205	-0.067421	3.415490
352.751939	3962.087789	16.853210	-0.067521	3.412118
352.862602	3954.030037	16.858215	-0.067536	3.408734
352.656641	3946.096808	16.863219	-0.067492	3.405388
352.731188	3938.140230	16.868224	-0.067501	3.402039
352.681265	3930.162097	16.873229	-0.067486	3.398674
352.913645	3922.156704	16.878234	-0.067524	3.395303
352.459089	3914.163279	16.883239	-0.067434	3.391909
352.429493	3906.148270	16.888243	-0.067424	3.388519
352.561379	3898.097201	16.893248	-0.067443	3.385115
352.156983	3890.218925	16.898253	-0.067362	3.381762
352.297568	3882.227305	16.903258	-0.067383	3.378377
352.399994	3874.187410	16.908263	-0.067397	3.374967
352.266831	3866.211268	16.913267	-0.067367	3.371572
352.003776	3858.242784	16.918272	-0.067313	3.368171
352.186595	3850.160845	16.923277	-0.067342	3.364736
351.798256	3842.320651	16.928282	-0.067264	3.361379
351.738831	3834.295185	16.933287	-0.067248	3.357951
352.025354	3826.254911	16.938291	-0.067296	3.354527
351.943063	3818.302558	16.943296	-0.067275	3.351123
351.574917	3810.306971	16.948301	-0.067202	3.347687
351.437395	3802.326358	16.953306	-0.067171	3.344261
351.598275	3794.329773	16.958311	-0.067195	3.340837
350.779722	3786.447775	16.963315	-0.067038	3.337421
351.207335	3778.344460	16.968320	-0.067112	3.333954
351.461042	3770.278638	16.973325	-0.067154	3.330493
351.588006	3762.293968	16.978330	-0.067172	3.327059
351.652964	3754.292639	16.983335	-0.067179	3.323611
351.421014	3746.374633	16.988339	-0.067131	3.320185
351.480009	3738.422894	16.993344	-0.067137	3.316751
351.081015	3730.423203	16.998349	-0.067057	3.313275
350.764670	3722.477974	17.003354	-0.066993	3.309823
350.992727	3714.390471	17.008359	-0.067030	3.306326
350.829901	3706.408675	17.013363	-0.066995	3.302856
350.946832	3698.423599	17.018368	-0.067011	3.299392
350.982901	3690.457802	17.023373	-0.067013	3.295930
350.619330	3682.502391	17.028378	-0.066940	3.292453
351.031069	3674.383037	17.033383	-0.067011	3.288931
351.130760	3666.420932	17.038387	-0.067024	3.285462
350.343695	3658.592148	17.043392	-0.066873	3.282012
349.526015	3650.655590	17.048397	-0.066715	3.278510
349.986778	3642.579447	17.053402	-0.066796	3.274994
349.714402	3634.594414	17.058407	-0.066740	3.271485
349.767669	3626.565183	17.063411	-0.066744	3.267966
349.899702	3618.539406	17.068416	-0.066764	3.264447
349.682120	3610.588077	17.073421	-0.066718	3.260944
349.853269	3602.561689	17.078426	-0.066744	3.257420
349.999564	3594.525683	17.083431	-0.066766	3.253886
350.291684	3586.517964	17.088435	-0.066815	3.250367
350.379107	3578.542906	17.093440	-0.066827	3.246851
350.353962	3570.536175	17.098445	-0.066817	3.243312
350.189161	3562.624697	17.103450	-0.066781	3.239805
350.213174	3554.652632	17.108455	-0.066780	3.236275
350.396714	3546.634068	17.113459	-0.066809	3.232728
349.916860	3538.705294	17.118464	-0.066714	3.229189
349.704335	3530.686355	17.123469	-0.066669	3.225617
349.601517	3522.715786	17.128474	-0.066645	3.222068
350.183889	3514.595602	17.133479	-0.066748	3.218476
350.080518	3506.640632	17.138483	-0.066724	3.214926
350.414645	3498.644977	17.143488	-0.066781	3.211372
350.083304	3490.687556	17.148493	-0.066714	3.207802
350.131961	3482.695698	17.153498	-0.066717	3.204230
350.247098	3474.729333	17.158503	-0.066734	3.200667
349.938391	3466.779925	17.163507	-0.066671	3.197091
349.752308	3458.811039	17.168512	-0.066631	3.193506
349.299608	3450.856165	17.173517	-0.066542	3.189912
349.398796	3442.850718	17.178522	-0.066555	3.186316
349.354107	3434.814199	17.183527	-0.066541	3.182695
349.493029	3426.811192	17.188531	-0.066562	3.179093
349.424529	3418.885819	17.193536	-0.066544	3.175513
348.905345	3410.914037	17.198541	-0.066442	3.171888
348.744241	3402.964149	17.203546	-0.066407	3.168285
348.426169	3394.943719	17.208551	-0.066342	3.164638
348.880908	3386.911753	17.213555	-0.066422	3.161017
348.875508	3378.929980	17.218560	-0.066415	3.157393
348.840418	3370.890275	17.223565	-0.066403	3.153738
349.138152	3362.903113	17.228570	-0.066454	3.150118
348.897488	3354.907107	17.233575	-0.066404	3.146464
349.086834	3346.899020	17.238579	-0.066434	3.142821
348.864775	3338.984114	17.243584	-0.066387	3.139197
348.884695	3330.946486	17.248589	-0.066385	3.135524
348.921323	3322.992964	17.253594	-0.066387	3.131886
348.962371	3314.981485	17.258599	-0.066389	3.128218
349.082277	3306.947671	17.263603	-0.066406	3.124538
348.705498	3299.090701	17.268608	-0.066331	3.120912
348.698523	3291.079605	17.273613	-0.066325	3.117229
348.751012	3283.100457	17.278618	-0.066329	3.113558
348.366196	3275.122071	17.283623	-0.066252	3.109863
348.039302	3267.196865	17.288627	-0.066186	3.106191
347.869393	3259.232857	17.293632	-0.066149	3.102504
347.967087	3251.167561	17.298637	-0.066162	3.098778
348.340201	3243.118239	17.303642	-0.066226	3.095069
348.170076	3235.156004	17.308647	-0.066189	3.091369
348.189383	3227.143698	17.313651	-0.066188	3.087651
347.788211	3219.242499	17.318656	-0.066108	3.083959
347.584008	3211.278456	17.323661	-0.066065	3.080244
347.553553	3203.306942	17.328666	-0.066054	3.076529
347.427669	3195.257238	17.333671	-0.066025	3.072768
347.687834	3187.157585	17.338675	-0.066068	3.068998
347.541592	3179.243217	17.343680	-0.066036	3.065290
347.721977	3171.242696	17.348685	-0.066064	3.061554
347.632378	3163.267880	17.353690	-0.066042	3.057811
347.755701	3155.245508	17.358695	-0.066060	3.054052
347.816124	3147.282662	17.363699	-0.066066	3.050314
347.884367	3139.300879	17.368704	-0.066073	3.046562
347.730409	3131.345496	17.373709	-0.066039	3.042807
347.685314	3123.387290	17.378714	-0.066026	3.039052
347.648073	3115.408390	17.383719	-0.066013	3.035282
347.790800	3107.373654	17.388723	-0.066035	3.031490
347.872403	3099.384993	17.393728	-0.066045	3.027713
347.741133	3091.391853	17.398733	-0.066015	3.023918
347.431880	3083.523613	17.403738	-0.065952	3.020168
347.295129	3075.524911	17.408743	-0.065922	3.016361
347.415929	3067.497260	17.413747	-0.065939	3.012547
347.185842	3059.533371	17.418752	-0.065891	3.008742
347.222826	3051.508076	17.423757	-0.065892	3.004916
347.365836	3043.564647	17.428762	-0.065914	3.001130
347.315337	3035.578766	17.433767	-0.065899	2.997308
347.174183	3027.595205	17.438771	-0.065867	2.993479
347.147472	3019.616825	17.443776	-0.065857	2.989652
346.671814	3011.694298	17.448781	-0.065763	2.985825
346.748039	3003.670215	17.453786	-0.065772	2.981972
346.762875	2995.670213	17.458791	-0.065770	2.978122
346.925297	2987.652307	17.463795	-0.065795	2.974267
346.737214	2979.693627	17.468800	-0.065755	2.970417
346.948350	2971.634938	17.473805	-0.065789	2.966534
346.826232	2963.729282	17.478810	-0.065761	2.962703
346.769114	2955.748270	17.483815	-0.065745	2.958834
346.374376	2947.835099	17.488819	-0.065666	2.954975
346.384088	2939.824732	17.493824	-0.065663	2.951085
346.713087	2931.752159	17.498829	-0.065719	2.947177
346.470429	2923.839232	17.503834	-0.065668	2.943310
346.319051	2915.857713	17.508839	-0.065635	2.939410
346.748459	2907.840277	17.513843	-0.065709	2.935519
346.465771	2899.926976	17.518848	-0.065652	2.931635
346.052328	2891.946330	17.523853	-0.065569	2.927705
345.844603	2883.993346	17.528858	-0.065525	2.923795
346.092999	2875.955494	17.533863	-0.065566	2.919863
345.960196	2868.003614	17.538867	-0.065537	2.915947
346.024809	2859.958790	17.543872	-0.065543	2.911991
346.036793	2851.920593	17.548877	-0.065540	2.908030
346.068652	2843.937273	17.553882	-0.065541	2.904092
345.919044	2836.003968	17.558887	-0.065508	2.900163
345.316861	2828.122662	17.563891	-0.065390	2.896229
345.476583	2820.090210	17.568896	-0.065415	2.892257
345.309768	2812.102843	17.573901	-0.065379	2.888284
345.760554	2804.055231	17.578906	-0.065457	2.884310
345.755544	2796.111811	17.583911	-0.065451	2.880357
345.335684	2788.212954	17.588915	-0.065368	2.876397
345.165718	2780.250067	17.593920	-0.065331	2.872414
345.139336	2772.230241	17.598925	-0.065321	2.868405
345.058487	2764.240288	17.603930	-0.065300	2.864402
345.305023	2756.239923	17.608935	-0.065341	2.860408
345.256350	2748.263674	17.613939	-0.065327	2.856402
344.945078	2740.321120	17.618944	-0.065264	2.852393
344.416341	2732.376294	17.623949	-0.065160	2.848365
344.489847	2724.358021	17.628954	-0.065168	2.844329
344.497986	2716.415454	17.633959	-0.065165	2.840321
344.284329	2708.450281	17.638963	-0.065120	2.836283
343.955174	2700.504911	17.643968	-0.065053	2.832243
343.911926	2692.453191	17.648973	-0.065040	2.828160
343.965106	2684.448717	17.653978	-0.065044	2.824100
344.160375	2676.432554	17.658983	-0.065075	2.820037
344.076936	2668.486444	17.663987	-0.065055	2.815988
344.169008	2660.485563	17.668992	-0.065067	2.811915
343.588938	2652.566319	17.673997	-0.064953	2.807838
343.760793	2644.555582	17.679002	-0.064980	2.803753
344.016869	2636.546612	17.684007	-0.065022	2.799667
344.411471	2628.533024	17.689011	-0.065091	2.795582
343.801406	2620.673266	17.694016	-0.064972	2.791510
343.956217	2612.621713	17.699021	-0.064995	2.787379
343.733979	2604.720725	17.704026	-0.064949	2.783297
343.419378	2596.763665	17.709031	-0.064885	2.779174
343.416387	2588.774678	17.714035	-0.064879	2.775047
343.924440	2580.705387	17.719040	-0.064969	2.770904
343.787050	2572.746949	17.724045	-0.064938	2.766772
343.241930	2564.872129	17.729050	-0.064831	2.762653
343.265148	2556.865206	17.734055	-0.064830	2.758494
342.992037	2548.918083	17.739059	-0.064774	2.754342
342.878477	2540.902489	17.744064	-0.064748	2.750157
342.542427	2532.943566	17.749069	-0.064680	2.745981
343.316818	2524.842494	17.754074	-0.064819	2.741795
342.998333	2516.924947	17.759079	-0.064754	2.737629
342.995814	2508.950909	17.764083	-0.064748	2.733448
342.729027	2501.030824	17.769088	-0.064694	2.729271
342.414747	2493.056945	17.774093	-0.064630	2.725057
342.640627	2485.082190	17.779098	-0.064667	2.720870
343.148930	2477.016411	17.784103	-0.064756	2.716647
342.878289	2469.096925	17.789107	-0.064700	2.712445
342.699755	2461.142199	17.794112	-0.064662	2.708223
342.403553	2453.183016	17.799117	-0.064601	2.703985
342.581961	2445.208370	17.804122	-0.064629	2.699762
342.608700	2437.221084	17.809127	-0.064629	2.695517
342.189194	2429.303517	17.814131	-0.064546	2.691273
341.990175	2421.355470	17.819136	-0.064504	2.687020
342.104259	2413.322982	17.824141	-0.064520	2.682736
342.610046	2405.279916	17.829146	-0.064608	2.678464
342.576237	2397.315949	17.834151	-0.064597	2.674193
342.411614	2389.376094	17.839155	-0.064561	2.669920
342.139783	2381.444791	17.844160	-0.064505	2.665637
342.239535	2373.428030	17.849165	-0.064519	2.661326
342.478117	2365.447014	17.854170	-0.064558	2.657037
342.237023	2357.499181	17.859175	-0.064508	2.652726
342.361782	2349.470829	17.864179	-0.064526	2.648389
342.570708	2341.474778	17.869184	-0.064559	2.644069
342.056999	2333.630272	17.874189	-0.064458	2.639775
342.420259	2325.619233	17.879194	-0.064521	2.635442
341.954622	2317.692901	17.884199	-0.064429	2.631092
342.010357	2309.684789	17.889203	-0.064434	2.626726
341.884004	2301.746314	17.894208	-0.064405	2.622379
341.895041	2293.754076	17.899213	-0.064402	2.618004
341.828147	2285.819056	17.904218	-0.064384	2.613647
341.949793	2277.781993	17.909223	-0.064402	2.609241
341.847428	2269.823929	17.914227	-0.064377	2.604854
342.182146	2261.861514	17.919232	-0.064434	2.600489
341.752319	2253.951063	17.924237	-0.064349	2.596091
341.596085	2245.919699	17.929242	-0.064315	2.591639
341.356697	2237.903426	17.934247	-0.064265	2.587181
341.665528	2229.897050	17.939251	-0.064317	2.582759
341.809666	2221.938219	17.944256	-0.064339	2.578345
341.591880	2213.992577	17.949261	-0.064293	2.573905
341.663547	2206.028232	17.954266	-0.064301	2.569467
341.380891	2198.113701	17.959271	-0.064243	2.565024
340.985912	2190.209515	17.964275	-0.064165	2.560571
341.144312	2182.217891	17.969280	-0.064189	2.556101
341.076801	2174.234562	17.974285	-0.064171	2.551612
340.940956	2166.283757	17.979290	-0.064141	2.547128
340.522200	2158.368876	17.984295	-0.064057	2.542636
340.770155	2150.337152	17.989299	-0.064098	2.538118
340.357253	2142.449120	17.994304	-0.064016	2.533625
340.494110	2134.392325	17.999309	-0.064036	2.529069
341.001058	2126.346776	18.004314	-0.064125	2.524538
341.107885	2118.396869	18.009319	-0.064140	2.520024
340.715958	2110.511626	18.014323	-0.064062	2.515502
340.522820	2102.574908	18.019328	-0.064021	2.510957
340.699178	2094.542332	18.024333	-0.064048	2.506377
340.401629	2086.631298	18.029338	-0.063988	2.501822
340.570035	2078.610151	18.034343	-0.064014	2.497231
340.655760	2070.656176	18.039347	-0.064025	2.492664
340.446166	2062.728150	18.044352	-0.063980	2.488081
340.359171	2054.735077	18.049357	-0.063959	2.483461
340.129040	2046.858443	18.054362	-0.063911	2.478889
339.833803	2038.937969	18.059367	-0.063851	2.474278
339.607259	2030.972374	18.064371	-0.063803	2.469638
339.614360	2022.966792	18.069376	-0.063799	2.464983
339.649718	2014.986790	18.074381	-0.063801	2.460337
339.700199	2007.012626	18.079386	-0.063805	2.455686
339.610592	1999.054675	18.084391	-0.063783	2.451026
339.349527	1991.116728	18.089395	-0.063729	2.446355
339.548296	1983.110680	18.094400	-0.063761	2.441670
339.177034	1975.219519	18.099405	-0.063686	2.437000
339.629789	1967.155776	18.104410	-0.063765	2.432283
339.771916	1959.135181	18.109415	-0.063787	2.427559
339.523474	1951.228472	18.114419	-0.063735	2.422862
339.545182	1943.278618	18.119424	-0.063734	2.418151
339.770835	1935.271585	18.124429	-0.063771	2.413414
339.161566	1927.438621	18.129434	-0.063652	2.408704
339.330191	1919.407390	18.134439	-0.063678	2.403929
339.087063	1911.501744	18.139443	-0.063628	2.399187
338.901009	1903.591973	18.144448	-0.063588	2.394437
338.588113	1895.649542	18.149453	-0.063524	2.389648
338.662034	1887.632235	18.154458	-0.063533	2.384835
338.260279	1879.755513	18.159463	-0.063453	2.380059
338.505770	1871.724264	18.164467	-0.063493	2.375233
338.489094	1863.768079	18.169472	-0.063485	2.370420
338.361270	1855.815818	18.174477	-0.063456	2.365591
338.540683	1847.831279	18.179482	-0.063484	2.360758
338.223230	1839.948109	18.184487	-0.063420	2.355936
337.979156	1832.005819	18.189491	-0.063369	2.351074
338.098310	1824.014318	18.194496	-0.063386	2.346202
338.231011	1815.992393	18.199501	-0.063406	2.341302
338.405366	1808.030786	18.204506	-0.063433	2.336432
338.583817	1800.051607	18.209511	-0.063461	2.331542
338.362479	1792.117706	18.214515	-0.063414	2.326636
337.791608	1784.287505	18.219520	-0.063303	2.321754
338.200839	1776.241263	18.224525	-0.063374	2.316811
338.285678	1768.285937	18.229530	-0.063384	2.311886
337.559385	1760.436846	18.234535	-0.063244	2.306947
337.476617	1752.486255	18.239539	-0.063223	2.301990
337.324326	1744.563685	18.244544	-0.063190	2.297033
337.315912	1736.574577	18.249549	-0.063183	2.292037
337.187022	1728.642704	18.254554	-0.063154	2.287055
338.078280	1720.497857	18.259559	-0.063314	2.282017
337.816454	1712.649877	18.264563	-0.063260	2.277054
337.708360	1704.704610	18.269568	-0.063235	2.272032
337.623748	1696.711795	18.274573	-0.063214	2.266971
337.649530	1688.758393	18.279578	-0.063214	2.261934
337.296848	1680.873063	18.284583	-0.063143	2.256895
337.417533	1672.878392	18.289587	-0.063160	2.251817
337.149288	1665.000592	18.294592	-0.063105	2.246768
336.807439	1657.073930	18.299597	-0.063036	2.241669
337.189959	1649.054345	18.304602	-0.063102	2.236565
337.608932	1641.046689	18.309607	-0.063175	2.231459
337.413679	1633.130194	18.314611	-0.063133	2.226345
337.602172	1625.178641	18.319616	-0.063163	2.221232
337.656935	1617.223624	18.324621	-0.063168	2.216092
337.666099	1609.317265	18.329626	-0.063165	2.210968
337.311286	1601.419298	18.334631	-0.063093	2.205803
337.020671	1593.533121	18.339635	-0.063034	2.200640
336.961440	1585.601992	18.344640	-0.063018	2.195457
336.609884	1577.671594	18.349645	-0.062947	2.190235
336.171642	1569.777913	18.354650	-0.062860	2.185017
336.195923	1561.804045	18.359655	-0.062860	2.179776
335.587396	1553.938669	18.364659	-0.062741	2.174535
335.763447	1545.926536	18.369664	-0.062769	2.169258
335.976204	1537.891540	18.374669	-0.062803	2.163957
336.204189	1529.929064	18.379674	-0.062840	2.158692
336.086426	1522.021843	18.384679	-0.062813	2.153418
336.294424	1514.028842	18.389683	-0.062846	2.148105
336.753719	1506.035146	18.394688	-0.062927	2.142803
335.770246	1498.281016	18.399693	-0.062738	2.137509
335.908863	1490.312829	18.404698	-0.062759	2.132166
335.696822	1482.387601	18.409703	-0.062714	2.126805
335.458819	1474.484864	18.414707	-0.062665	2.121443
335.709631	1466.490048	18.419712	-0.062706	2.116053
335.635429	1458.517288	18.424717	-0.062687	2.110632
335.665419	1450.559078	18.429722	-0.062688	2.105218
335.709636	1442.615348	18.434727	-0.062691	2.099800
335.531287	1434.697578	18.439731	-0.062652	2.094365
336.072247	1426.687446	18.444736	-0.062748	2.088923
335.381080	1418.885297	18.449741	-0.062614	2.083487
335.573654	1410.935297	18.454746	-0.062644	2.078024
335.788138	1402.968108	18.459751	-0.062679	2.072536
335.691392	1395.036407	18.464755	-0.062656	2.067027
336.072612	1387.058913	18.469760	-0.062722	2.061521
335.901055	1379.176471	18.474765	-0.062685	2.056009
335.791737	1371.259055	18.479770	-0.062659	2.050464
335.647870	1363.362198	18.484775	-0.062627	2.044915
335.387950	1355.478469	18.489779	-0.062573	2.039349
334.989208	1347.646460	18.494784	-0.062494	2.033788
334.876511	1339.676267	18.499789	-0.062468	2.028145
334.972953	1331.706814	18.504794	-0.062480	2.022508
334.721013	1323.833943	18.509799	-0.062428	2.016888
334.636682	1315.880643	18.514803	-0.062407	2.011212
334.322504	1307.989891	18.519808	-0.062344	2.005541
334.132907	1300.074428	18.524813	-0.062303	1.999849
334.445678	1292.109797	18.529818	-0.062356	1.994159
334.522302	1284.144024	18.534823	-0.062365	1.988426
333.840710	1276.315493	18.539827	-0.062233	1.982694
334.092905	1268.352367	18.544832	-0.062275	1.976950
333.944581	1260.426478	18.549837	-0.062242	1.971172
333.884175	1252.501754	18.554842	-0.062226	1.965387
334.296837	1244.515483	18.559847	-0.062297	1.959592
334.046088	1236.661357	18.564851	-0.062245	1.953804
334.236566	1228.718907	18.569856	-0.062276	1.947983
333.758866	1220.848346	18.574861	-0.062182	1.942123
333.884696	1212.918182	18.579866	-0.062200	1.936268
334.200020	1204.928004	18.584871	-0.062253	1.930372
333.411876	1197.152991	18.589875	-0.062101	1.924494
333.707691	1189.197434	18.594880	-0.062151	1.918586
333.840123	1181.229927	18.599885	-0.062171	1.912632
333.599069	1173.352731	18.604890	-0.062121	1.906685
333.559757	1165.434248	18.609895	-0.062108	1.900711
333.037278	1157.625158	18.614899	-0.062006	1.894745
333.382689	1149.623902	18.619904	-0.062065	1.888715
332.931303	1141.772781	18.624909	-0.061975	1.882687
332.869956	1133.899787	18.629914	-0.061959	1.876669
332.915354	1125.955562	18.634919	-0.061962	1.870589
333.234489	1117.961678	18.639923	-0.062016	1.864484
333.297361	1110.069764	18.644928	-0.062023	1.858407
333.714494	1102.078835	18.649933	-0.062095	1.852275
333.640889	1094.204695	18.654938	-0.062076	1.846155
333.211754	1086.418648	18.659943	-0.061991	1.840041
332.882157	1078.569271	18.664947	-0.061925	1.833869
332.726387	1070.697275	18.669952	-0.061891	1.827679
332.225570	1062.859617	18.674957	-0.061792	1.821453
331.905080	1054.990856	18.679962	-0.061727	1.815203
332.426475	1046.964490	18.684967	-0.061819	1.808910
332.340238	1039.076860	18.689971	-0.061798	1.802631
332.368117	1031.190231	18.694976	-0.061798	1.796344
332.438437	1023.236538	18.699981	-0.061806	1.789987
332.321893	1015.369962	18.704986	-0.061779	1.783654
332.288589	1007.478781	18.709991	-0.061767	1.777288
332.163620	999.601847	18.714995	-0.061739	1.770900
332.224419	991.711129	18.720000	-0.061745	1.764501
331.979756	983.877223	18.725005	-0.061694	1.758087
332.301201	975.919384	18.730010	-0.061749	1.751619
332.509332	968.000758	18.735015	-0.061783	1.745146
332.309826	960.169231	18.740019	-0.061740	1.738668
332.099257	952.339948	18.745024	-0.061696	1.732165
331.871254	944.469199	18.750029	-0.061648	1.725601
331.513302	936.682329	18.755034	-0.061577	1.719066
331.428355	928.800520	18.760039	-0.061556	1.712461
331.136913	920.940955	18.765043	-0.061496	1.705822
331.534236	912.980898	18.770048	-0.061565	1.699165
331.290569	905.131939	18.775053	-0.061514	1.692489
331.294468	897.255256	18.780058	-0.061510	1.685797
331.617678	889.332063	18.785063	-0.061565	1.679081
331.773828	881.436904	18.790067	-0.061589	1.672340
331.764100	873.583996	18.795072	-0.061582	1.665586
331.171217	865.844804	18.800077	-0.061466	1.658822
331.103180	857.989315	18.805082	-0.061448	1.652001
331.393207	850.048428	18.810087	-0.061497	1.645128
331.174695	842.250539	18.815091	-0.061451	1.638280
331.370275	834.339988	18.820096	-0.061483	1.631362
331.032409	826.502990	18.825101	-0.061415	1.624405
330.639881	818.729387	18.830106	-0.061336	1.617466
330.852565	810.812384	18.835111	-0.061371	1.610455
331.213605	802.889294	18.840115	-0.061433	1.603430
331.007907	795.105449	18.845120	-0.061389	1.596418
330.570511	787.329182	18.850125	-0.061303	1.589347
330.413543	779.500151	18.855130	-0.061268	1.582238
330.337103	771.657755	18.860135	-0.061249	1.575097
330.184449	763.823702	18.865139	-0.061215	1.567919
330.599156	755.904339	18.870144	-0.061287	1.560714
330.076485	748.172684	18.875149	-0.061185	1.553509
330.230556	740.287811	18.880154	-0.061209	1.546230
330.323716	732.447698	18.885159	-0.061221	1.538949
329.983578	724.668541	18.890163	-0.061152	1.531624
329.856762	716.862633	18.895168	-0.061124	1.524272
329.666672	709.057915	18.900173	-0.061083	1.516875
330.260735	701.123109	18.905178	-0.061188	1.509440
329.817913	693.385196	18.910183	-0.061101	1.501995
329.314990	685.647646	18.915187	-0.061002	1.494503
329.212626	677.839119	18.920192	-0.060978	1.486969
329.354810	669.982125	18.925197	-0.060999	1.479387
329.563280	662.108625	18.930202	-0.061033	1.471761
329.144012	654.370206	18.935207	-0.060950	1.464127
328.477747	646.676161	18.940211	-0.060821	1.456456
328.633019	638.829976	18.945216	-0.060844	1.448728
328.373013	631.045772	18.950221	-0.060791	1.440952
327.994295	623.331052	18.955226	-0.060715	1.433184
328.855397	615.321556	18.960231	-0.060870	1.425282
328.756271	607.568342	18.965235	-0.060847	1.417436
329.153103	599.718675	18.970240	-0.060915	1.409531
328.580656	592.054362	18.975245	-0.060804	1.401607
328.606934	584.288467	18.980250	-0.060804	1.393635
328.560476	576.510229	18.985255	-0.060790	1.385593
328.586735	568.727073	18.990259	-0.060790	1.377510
328.448255	560.982637	18.995264	-0.060759	1.369392
328.158109	553.276921	19.000269	-0.060700	1.361240
327.967091	545.557950	19.005274	-0.060659	1.353041
327.881937	537.794908	19.010279	-0.060638	1.344765
327.902030	530.022034	19.015283	-0.060637	1.336446
327.729402	522.318496	19.020288	-0.060599	1.328114
327.625012	514.587353	19.025293	-0.060575	1.319713
328.369785	506.662440	19.030298	-0.060708	1.311201
328.436150	498.888103	19.035303	-0.060716	1.302674
328.576630	491.143614	19.040307	-0.060737	1.294139
328.008754	483.558005	19.045312	-0.060626	1.285590
327.981291	475.854276	19.050317	-0.060616	1.276954
327.641144	468.219839	19.055322	-0.060547	1.268278
327.562819	460.511651	19.060327	-0.060528	1.259508
327.710974	452.775073	19.065331	-0.060550	1.250688
327.731238	445.088190	19.070336	-0.060549	1.241838
327.212824	437.495131	19.075341	-0.060447	1.232927
327.591320	429.719503	19.080346	-0.060513	1.223915
328.257390	421.923003	19.085351	-0.060632	1.214870
327.991905	414.311899	19.090355	-0.060577	1.205790
328.043887	406.672289	19.095360	-0.060582	1.196671
327.335443	399.142930	19.100365	-0.060445	1.187458
327.590560	391.445281	19.105370	-0.060488	1.178169
327.124151	383.896784	19.110375	-0.060396	1.168837
326.901149	376.288913	19.115379	-0.060349	1.159408
327.002675	368.625930	19.120384	-0.060363	1.149903
326.450085	361.081466	19.125389	-0.060255	1.140326
326.788399	353.386570	19.130394	-0.060313	1.130671
325.995093	345.926050	19.135399	-0.060161	1.120984
326.037445	338.305938	19.140403	-0.060163	1.111192
326.098390	330.695159	19.145408	-0.060170	1.101329
325.982545	323.123162	19.150413	-0.060143	1.091388
326.304791	315.490329	19.155418	-0.060198	1.081375
326.369117	307.924274	19.160423	-0.060205	1.071298
326.446877	300.352069	19.165427	-0.060215	1.061121
326.442869	292.826107	19.170432	-0.060209	1.050889
326.254097	285.333438	19.175437	-0.060169	1.040558
325.985282	277.880412	19.180442	-0.060114	1.030159
325.996872	270.374048	19.185447	-0.060111	1.019647
325.668984	262.934790	19.190451	-0.060045	1.009038
326.046131	255.394762	19.195456	-0.060110	0.998347
325.667173	247.973217	19.200461	-0.060035	0.987521
325.619604	240.527426	19.205466	-0.060021	0.976625
325.490384	233.109065	19.210471	-0.059992	0.965625
325.232243	225.727678	19.215475	-0.059939	0.954519
325.456865	218.284524	19.220480	-0.059976	0.943318
324.869229	211.000149	19.225485	-0.059862	0.932007
325.358626	203.530349	19.230490	-0.059948	0.920563
325.055095	196.235649	19.235495	-0.059887	0.909031
325.073320	188.884261	19.240499	-0.059886	0.897351
324.930968	181.594857	19.245504	-0.059854	0.885571
324.707391	174.338232	19.250509	-0.059808	0.873663
325.165823	166.972903	19.255514	-0.059888	0.861609
325.050039	159.757784	19.260519	-0.059862	0.849467
324.879882	152.560511	19.265523	-0.059826	0.837163
324.866461	145.343388	19.270528	-0.059818	0.824689
324.283137	138.271562	19.275533	-0.059705	0.812103
324.253144	131.118553	19.280538	-0.059695	0.799347
324.731216	123.905564	19.285543	-0.059779	0.786440
324.102568	116.931392	19.290547	-0.059657	0.773397
324.279335	109.837493	19.295552	-0.059686	0.760173
323.913983	102.869845	19.300557	-0.059613	0.746772
323.796934	95.888736	19.305562	-0.059587	0.733187
323.981060	88.892807	19.310567	-0.059616	0.719423
323.743302	82.012834	19.315571	-0.059568	0.705473
323.956910	75.276519	19.320576	-0.059603	0.691707