Mon Apr 19 09:29:45 2021

Number of Points = 3630
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.105319	0.154076	0.000000	0.000088	0.312942

2.934135	0.195259	0.005005	0.000120	0.312989
3.019899	0.181553	0.010010	0.000104	0.312998
3.260805	0.133993	0.015014	0.000059	0.312980
3.004182	0.182424	0.020019	0.000107	0.312989
2.930997	0.196399	0.025024	0.000120	0.312992
3.113098	0.160493	0.030029	0.000086	0.312979
2.936717	0.196909	0.035034	0.000119	0.312999
2.484347	0.279053	0.040038	0.000203	0.312999
3.324077	0.088525	0.045043	0.000047	0.312823
3.165980	0.079040	0.050048	0.000077	0.312647
3.232788	0.065798	0.055053	0.000064	0.312642
3.169248	0.078607	0.060058	0.000076	0.312648
2.934666	0.121114	0.065062	0.000120	0.312647
2.735772	0.160039	0.070067	0.000157	0.312660
2.841862	0.139951	0.075072	0.000137	0.312656
2.842994	0.139138	0.080077	0.000137	0.312654
3.282151	0.059167	0.085082	0.000055	0.312653
2.805008	0.143775	0.090086	0.000144	0.312643
3.020216	0.104830	0.095091	0.000104	0.312644
3.006660	0.106888	0.100096	0.000106	0.312642
2.791009	0.079293	0.105101	0.000146	0.312333
2.662828	0.106077	0.110106	0.000170	0.312349
2.949604	0.049697	0.115110	0.000117	0.312330
2.762150	0.087544	0.120115	0.000152	0.312347
2.991888	0.043873	0.125120	0.000109	0.312338
2.601231	0.117701	0.130125	0.000182	0.312352
2.735709	0.080452	0.135130	0.000156	0.312292
2.538725	0.058273	0.140134	0.000193	0.312024
2.666242	0.035679	0.145139	0.000169	0.312027
2.800936	0.011457	0.150144	0.000144	0.312028
2.732835	0.022886	0.155149	0.000157	0.312023
2.983025	-0.022015	0.160154	0.000110	0.312026
3.031531	-0.097922	0.165158	0.000101	0.311715
3.393296	-0.164378	0.170163	0.000034	0.311712
3.189349	-0.126401	0.175168	0.000072	0.311716
2.886792	-0.077231	0.180173	0.000128	0.311689
2.931286	-0.148578	0.185178	0.000120	0.311395
2.700046	-0.108465	0.190182	0.000163	0.311387
2.912610	-0.146281	0.195187	0.000124	0.311390
3.059006	-0.197715	0.200192	0.000096	0.311275
2.747319	-0.182404	0.205197	0.000154	0.311083
2.884349	-0.205961	0.210202	0.000129	0.311089
3.065494	-0.245462	0.215206	0.000095	0.311059
2.902571	-0.276055	0.220211	0.000125	0.310779
3.016097	-0.298261	0.225216	0.000104	0.310771
3.126984	-0.324686	0.230221	0.000084	0.310742
3.157183	-0.377712	0.235226	0.000078	0.310521
2.915727	-0.334296	0.240230	0.000123	0.310519
2.837599	-0.339933	0.245235	0.000138	0.310426
2.946998	-0.414308	0.250240	0.000117	0.310172
2.645410	-0.359610	0.255245	0.000173	0.310172
2.951321	-0.450563	0.260250	0.000116	0.310007
3.059091	-0.505026	0.265254	0.000096	0.309844
3.150308	-0.525114	0.270259	0.000079	0.309828
3.072125	-0.576667	0.275264	0.000094	0.309521
3.009668	-0.566513	0.280269	0.000106	0.309515
3.133910	-0.630364	0.285274	0.000082	0.309322
2.971429	-0.620478	0.290278	0.000113	0.309230
2.587474	-0.575182	0.295283	0.000184	0.309116
2.844616	-0.666076	0.300288	0.000136	0.308909
2.882111	-0.685378	0.305293	0.000129	0.308851
2.895843	-0.742008	0.310298	0.000127	0.308597
2.705155	-0.708648	0.315302	0.000162	0.308591
2.528178	-0.741434	0.320307	0.000195	0.308287
2.885654	-0.809774	0.325312	0.000129	0.308271
2.945726	-0.876370	0.330317	0.000118	0.308010
3.003912	-0.892168	0.335322	0.000107	0.307985
2.727274	-0.909416	0.340326	0.000158	0.307668
2.626217	-0.896395	0.345331	0.000177	0.307643
2.435050	-0.922618	0.350336	0.000213	0.307356
2.514499	-0.943267	0.355341	0.000198	0.307327
2.808976	-1.062571	0.360346	0.000143	0.307017
2.515631	-1.018160	0.365350	0.000198	0.306975
2.764441	-1.117861	0.370355	0.000151	0.306718
3.036910	-1.190151	0.375360	0.000101	0.306611
2.790183	-1.195806	0.380365	0.000147	0.306373
2.662708	-1.206171	0.385370	0.000170	0.306214
2.497586	-1.205335	0.390374	0.000201	0.306077
2.379000	-1.236631	0.395379	0.000223	0.305827
2.695017	-1.314624	0.400384	0.000164	0.305729
2.174723	-1.268520	0.405389	0.000261	0.305500
1.831338	-1.229198	0.410394	0.000325	0.305391
1.733147	-1.260466	0.415398	0.000343	0.305158
2.473901	-1.438281	0.420403	0.000205	0.304953
2.245993	-1.422170	0.425408	0.000248	0.304833
2.113200	-1.466297	0.430413	0.000273	0.304509
2.668455	-1.589421	0.435418	0.000169	0.304404
2.374561	-1.575238	0.440422	0.000224	0.304217
2.348191	-1.628420	0.445427	0.000229	0.303942
2.273103	-1.645419	0.450432	0.000243	0.303796
2.425998	-1.721750	0.455437	0.000215	0.303565
2.517210	-1.789135	0.460442	0.000198	0.303322
2.348572	-1.794321	0.465446	0.000229	0.303151
2.486104	-1.860244	0.470451	0.000203	0.302956
2.116631	-1.856446	0.475456	0.000272	0.302654
1.556138	-1.790331	0.480461	0.000376	0.302483
1.884712	-1.885311	0.485466	0.000315	0.302314
1.974138	-1.968248	0.490470	0.000299	0.301995
2.145815	-2.033093	0.495475	0.000267	0.301834
2.063176	-2.055789	0.500480	0.000282	0.301653
2.124264	-2.129911	0.505485	0.000271	0.301350
1.634437	-2.085186	0.510490	0.000362	0.301138
1.361922	-2.075240	0.515494	0.000413	0.300948
1.538052	-2.150988	0.520499	0.000380	0.300737
1.264674	-2.147013	0.525504	0.000431	0.300517
1.025606	-2.145720	0.530509	0.000475	0.300315
1.469689	-2.269004	0.535514	0.000393	0.300109
1.039291	-2.248197	0.540518	0.000473	0.299833
1.187393	-2.328779	0.545523	0.000445	0.299574
1.018916	-2.334925	0.550528	0.000477	0.299396
0.716166	-2.320410	0.555533	0.000533	0.299200
0.509702	-2.347393	0.560538	0.000571	0.298888
0.323868	-2.357304	0.565542	0.000606	0.298677
-0.053618	-2.326177	0.570547	0.000676	0.298495
-0.485456	-2.296264	0.575552	0.000757	0.298260
-0.533682	-2.336244	0.580557	0.000766	0.298023
-0.646440	-2.348563	0.585562	0.000787	0.297864
-1.395163	-2.259848	0.590566	0.000926	0.297634
-1.456985	-2.300045	0.595571	0.000938	0.297384
-1.482165	-2.324683	0.600576	0.000942	0.297242
-1.899037	-2.302303	0.605581	0.001020	0.296982
-1.766707	-2.365624	0.610586	0.000995	0.296790
-2.091741	-2.335820	0.615590	0.001056	0.296648
-2.421050	-2.334207	0.620595	0.001117	0.296364
-2.722143	-2.312338	0.625600	0.001173	0.296203
-3.443555	-2.210115	0.630605	0.001307	0.296062
-3.359923	-2.278900	0.635610	0.001292	0.295800
-3.778967	-2.221645	0.640614	0.001370	0.295708
-4.055976	-2.213030	0.645619	0.001421	0.295504
-4.464257	-2.156277	0.650624	0.001497	0.295418
-4.568311	-2.191021	0.655629	0.001517	0.295155
-4.553600	-2.222366	0.660634	0.001514	0.295015
-5.307353	-2.116613	0.665638	0.001654	0.294861
-4.979044	-2.216528	0.670643	0.001593	0.294664
-5.239740	-2.197885	0.675648	0.001642	0.294523
-5.527604	-2.189016	0.680653	0.001695	0.294309
-5.490251	-2.210905	0.685658	0.001688	0.294235
-5.675054	-2.234600	0.690662	0.001723	0.293953
-6.121850	-2.165512	0.695667	0.001806	0.293894
-6.664525	-2.119201	0.700672	0.001907	0.293636
-7.073194	-2.054635	0.705677	0.001983	0.293588
-7.219831	-2.074890	0.710682	0.002010	0.293357
-7.286096	-2.080846	0.715686	0.002022	0.293268
-6.967828	-2.174810	0.720691	0.001963	0.293090
-7.575086	-2.086135	0.725696	0.002076	0.292983
-7.629828	-2.109570	0.730701	0.002086	0.292818
-7.215455	-2.221201	0.735706	0.002009	0.292639
-7.486637	-2.201093	0.740710	0.002060	0.292494
-8.350662	-2.079511	0.745715	0.002221	0.292319
-8.165970	-2.127611	0.750720	0.002186	0.292247
-8.420571	-2.134576	0.755725	0.002234	0.291983
-8.376510	-2.147499	0.760730	0.002225	0.291959
-8.649913	-2.151285	0.765734	0.002276	0.291694
-8.809469	-2.120150	0.770739	0.002306	0.291704
-8.997737	-2.145785	0.775744	0.002341	0.291407
-9.625373	-2.039368	0.780749	0.002458	0.291369
-9.748919	-2.049619	0.785754	0.002481	0.291207
-10.091761	-2.012120	0.790758	0.002545	0.291084
-9.869082	-2.065793	0.795763	0.002503	0.291018
-9.884872	-2.115997	0.800768	0.002506	0.290754
-9.666284	-2.158763	0.805773	0.002465	0.290739
-10.139062	-2.116075	0.810778	0.002553	0.290524
-10.355287	-2.082716	0.815782	0.002594	0.290494
-10.248776	-2.142329	0.820787	0.002574	0.290294
-10.576414	-2.111031	0.825792	0.002635	0.290153
-10.737037	-2.100691	0.830797	0.002665	0.290059
-10.947993	-2.107570	0.835802	0.002704	0.289833
-10.852685	-2.126936	0.840806	0.002686	0.289823
-10.909845	-2.178226	0.845811	0.002697	0.289515
-10.989604	-2.166687	0.850816	0.002712	0.289500
-11.057800	-2.195553	0.855821	0.002724	0.289294
-11.602362	-2.111457	0.860826	0.002826	0.289219
-11.686779	-2.120151	0.865830	0.002842	0.289099
-11.621991	-2.177387	0.870835	0.002829	0.288871
-11.913368	-2.122689	0.875840	0.002884	0.288880
-12.197446	-2.134397	0.880845	0.002937	0.288563
-12.025143	-2.164340	0.885850	0.002904	0.288570
-12.477832	-2.122218	0.890854	0.002989	0.288368
-13.048936	-2.040941	0.895859	0.003095	0.288255
-12.933921	-2.065967	0.900864	0.003074	0.288234
-13.330549	-2.046910	0.905869	0.003147	0.287968
-13.523939	-2.008757	0.910874	0.003183	0.287983
-13.612872	-2.025998	0.915878	0.003200	0.287815
-13.751155	-2.037722	0.920883	0.003226	0.287630
-13.794055	-2.027822	0.925888	0.003234	0.287641
-13.908881	-2.062802	0.930893	0.003255	0.287359
-14.060495	-2.042298	0.935898	0.003283	0.287324
-14.281018	-2.015741	0.940902	0.003324	0.287256
-14.944920	-1.944908	0.945907	0.003448	0.287005
-14.457255	-2.034665	0.950912	0.003357	0.286999
-13.979872	-2.154840	0.955917	0.003268	0.286831
-14.491047	-2.088685	0.960922	0.003363	0.286696
-14.629574	-2.064650	0.965926	0.003389	0.286690
-14.817627	-2.095297	0.970931	0.003424	0.286362
-14.975688	-2.064817	0.975936	0.003454	0.286371
-15.352762	-2.020536	0.980941	0.003524	0.286249
-15.435589	-2.040118	0.985946	0.003539	0.286074
-14.919313	-2.138377	0.990950	0.003443	0.286051
-15.486089	-2.088725	0.995955	0.003549	0.285781
-15.730788	-2.050507	1.000960	0.003594	0.285749
-15.852596	-2.040688	1.005965	0.003617	0.285687
-16.137708	-2.024588	1.010970	0.003670	0.285506
-16.241736	-2.008378	1.015974	0.003689	0.285492
-15.831468	-2.122539	1.020979	0.003613	0.285292
-15.950431	-2.132276	1.025984	0.003635	0.285133
-16.426735	-2.047614	1.030989	0.003724	0.285123
-16.062734	-2.172892	1.035994	0.003656	0.284823
-16.370426	-2.118057	1.040998	0.003713	0.284817
-16.677638	-2.099497	1.046003	0.003770	0.284628
-16.900469	-2.083445	1.051008	0.003812	0.284503
-17.216301	-2.025338	1.056013	0.003871	0.284507
-17.377089	-2.048216	1.061018	0.003900	0.284242
-17.800061	-1.976527	1.066022	0.003979	0.284215
-17.191973	-2.104455	1.071027	0.003866	0.284127
-17.365308	-2.122513	1.076032	0.003898	0.283874
-17.658674	-2.072020	1.081037	0.003953	0.283860
-17.935448	-2.057749	1.086042	0.004004	0.283676
-18.151592	-2.038128	1.091046	0.004045	0.283576
-18.488285	-1.975938	1.096051	0.004107	0.283581
-18.661724	-2.003420	1.101056	0.004140	0.283279
-18.731819	-1.996836	1.106061	0.004153	0.283248
-18.556862	-2.034848	1.111066	0.004120	0.283216
-19.060737	-1.992174	1.116070	0.004214	0.282966
-18.481257	-2.101697	1.121075	0.004106	0.282945
-18.509160	-2.126859	1.126080	0.004111	0.282790
-19.342311	-2.010582	1.131085	0.004266	0.282610
-19.334977	-2.007635	1.136090	0.004265	0.282632
-19.735911	-1.980244	1.141094	0.004339	0.282399
-19.839948	-1.978730	1.146099	0.004359	0.282310
-19.796554	-1.986165	1.151104	0.004351	0.282312
-19.601391	-2.082347	1.156109	0.004314	0.282001
-19.806327	-2.048184	1.161114	0.004353	0.281985
-20.477732	-1.935097	1.166118	0.004477	0.281939
-20.559886	-1.967395	1.171123	0.004493	0.281696
-20.131631	-2.042476	1.176128	0.004413	0.281711
-20.565044	-1.991091	1.181133	0.004494	0.281570
-21.124292	-1.927238	1.186138	0.004598	0.281375
-21.168811	-1.918526	1.191142	0.004606	0.281379
-20.713185	-2.033295	1.196147	0.004521	0.281214
-20.898677	-2.030196	1.201152	0.004556	0.281057
-21.122878	-1.989689	1.206157	0.004598	0.281055
-20.860601	-2.082301	1.211162	0.004549	0.280824
-21.674044	-1.949265	1.216166	0.004700	0.280747
-21.368263	-2.006619	1.221171	0.004643	0.280739
-21.432916	-2.037397	1.226176	0.004655	0.280519
-21.989262	-1.937845	1.231181	0.004759	0.280511
-21.862511	-1.975490	1.236186	0.004735	0.280436
-21.914839	-2.017036	1.241190	0.004745	0.280172
-21.750730	-2.048838	1.246195	0.004714	0.280162
-22.133058	-2.015553	1.251200	0.004786	0.279975
-22.174392	-2.035486	1.256205	0.004793	0.279833
-22.089158	-2.047244	1.261210	0.004777	0.279852
-22.570012	-2.021273	1.266214	0.004867	0.279534
-22.819499	-1.979582	1.271219	0.004913	0.279515
-22.358102	-2.075668	1.276224	0.004827	0.279452
-22.886147	-2.023005	1.281229	0.004926	0.279228
-23.142540	-1.974669	1.286234	0.004973	0.279237
-23.064249	-2.023940	1.291238	0.004959	0.279055
-23.386641	-1.996299	1.296243	0.005019	0.278894
-23.001687	-2.067517	1.301248	0.004947	0.278888
-23.259679	-2.076786	1.306253	0.004995	0.278596
-23.076051	-2.114782	1.311258	0.004961	0.278572
-23.452520	-2.069346	1.316262	0.005031	0.278453
-24.054991	-1.995592	1.321267	0.005143	0.278267
-23.790970	-2.041753	1.326272	0.005094	0.278276
-24.107865	-2.025976	1.331277	0.005153	0.278059
-24.231610	-2.018686	1.336282	0.005176	0.277979
-24.013188	-2.064707	1.341286	0.005135	0.277947
-24.553448	-2.025375	1.346291	0.005236	0.277640
-25.001624	-1.942045	1.351296	0.005319	0.277649
-24.911222	-1.976396	1.356301	0.005303	0.277556
-24.879440	-2.025278	1.361306	0.005297	0.277331
-25.281745	-1.950642	1.366310	0.005371	0.277339
-25.555389	-1.932288	1.371315	0.005422	0.277175
-25.137884	-2.040672	1.376320	0.005345	0.277006
-25.558967	-1.964128	1.381325	0.005423	0.277005
-25.876676	-1.944240	1.386330	0.005482	0.276807
-26.300082	-1.883081	1.391334	0.005561	0.276725
-26.116727	-1.915925	1.396339	0.005527	0.276727
-26.418469	-1.906963	1.401344	0.005583	0.276487
-26.806846	-1.853880	1.406349	0.005655	0.276395
-26.620786	-1.886815	1.411354	0.005621	0.276400
-26.502955	-1.956516	1.416358	0.005599	0.276147
-26.738618	-1.928893	1.421363	0.005643	0.276067
-26.248210	-2.018451	1.426368	0.005551	0.276065
-26.680787	-1.999885	1.431373	0.005632	0.275750
-27.127249	-1.916039	1.436378	0.005715	0.275764
-27.240885	-1.903897	1.441382	0.005736	0.275720
-27.183347	-1.953640	1.446387	0.005725	0.275513
-26.914138	-2.002194	1.451392	0.005675	0.275515
-27.453955	-1.933896	1.456397	0.005776	0.275358
-27.115302	-2.032355	1.461402	0.005713	0.275165
-27.344363	-1.989989	1.466406	0.005755	0.275168
-27.646085	-1.984747	1.471411	0.005811	0.274907
-27.736894	-1.976800	1.476416	0.005828	0.274862
-27.769515	-1.982467	1.481421	0.005834	0.274801
-27.928932	-2.005990	1.486426	0.005864	0.274524
-27.804856	-2.030054	1.491430	0.005841	0.274517
-27.843701	-2.053668	1.496435	0.005848	0.274355
-28.456652	-1.964660	1.501440	0.005962	0.274236
-28.495718	-1.960758	1.506445	0.005970	0.274219
-28.202724	-2.068098	1.511450	0.005915	0.273934
-28.258552	-2.067626	1.516454	0.005925	0.273883
-28.573180	-2.033496	1.521459	0.005984	0.273761
-29.022914	-1.984062	1.526464	0.006068	0.273590
-28.557230	-2.071958	1.531469	0.005981	0.273573
-29.407587	-1.959465	1.536474	0.006139	0.273350
-29.662506	-1.926135	1.541478	0.006187	0.273281
-29.944851	-1.873308	1.546483	0.006239	0.273289
-29.435126	-2.021542	1.551488	0.006144	0.272994
-29.724932	-1.972116	1.556493	0.006198	0.272977
-29.313032	-2.071612	1.561498	0.006122	0.272847
-30.085248	-1.969581	1.566502	0.006265	0.272643
-30.530596	-1.885819	1.571507	0.006348	0.272658
-29.991520	-2.021602	1.576512	0.006248	0.272457
-30.498899	-1.952943	1.581517	0.006342	0.272332
-30.491782	-1.951435	1.586522	0.006341	0.272347
-30.796914	-1.956374	1.591526	0.006398	0.272025
-31.260377	-1.871207	1.596531	0.006484	0.272030
-31.361885	-1.856640	1.601536	0.006503	0.272009
-32.126916	-1.767821	1.606541	0.006645	0.271741
-31.649656	-1.852758	1.611546	0.006556	0.271751
-31.773328	-1.830671	1.616550	0.006579	0.271749
-32.030731	-1.847422	1.621555	0.006627	0.271410
-32.199779	-1.814158	1.626560	0.006659	0.271424
-32.116986	-1.832126	1.631565	0.006643	0.271409
-31.741120	-1.959989	1.636570	0.006574	0.271091
-32.105129	-1.892881	1.641574	0.006641	0.271096
-32.329513	-1.863627	1.646579	0.006683	0.271034
-32.265509	-1.919631	1.651584	0.006671	0.270797
-32.504810	-1.879770	1.656589	0.006716	0.270778
-31.912383	-2.011272	1.661594	0.006605	0.270651
-31.991215	-2.023441	1.666598	0.006620	0.270509
-32.670966	-1.898431	1.671603	0.006747	0.270516
-32.279647	-2.030902	1.676608	0.006674	0.270188
-32.293315	-2.034225	1.681613	0.006676	0.270157
-32.094836	-2.099311	1.686618	0.006639	0.270002
-32.710116	-2.018343	1.691622	0.006754	0.269836
-32.613857	-2.039982	1.696627	0.006736	0.269814
-32.357742	-2.142329	1.701632	0.006688	0.269514
-33.401461	-1.951646	1.706637	0.006882	0.269519
-33.259009	-2.010309	1.711642	0.006856	0.269343
-33.354946	-2.011957	1.716646	0.006874	0.269240
-33.654774	-1.964094	1.721651	0.006930	0.269205
-33.748414	-2.004246	1.726656	0.006947	0.268897
-33.838945	-1.987855	1.731661	0.006964	0.268897
-33.550547	-2.071478	1.736666	0.006910	0.268729
-34.287784	-1.963223	1.741670	0.007047	0.268590
-34.455845	-1.931307	1.746675	0.007079	0.268597
-34.149088	-2.044821	1.751680	0.007022	0.268286
-34.767698	-1.936962	1.756685	0.007137	0.268261
-34.630918	-1.978743	1.761690	0.007111	0.268169
-34.469873	-2.044867	1.766694	0.007081	0.267970
-34.875078	-1.970557	1.771699	0.007157	0.267974
-35.011305	-1.997189	1.776704	0.007182	0.267696
-35.225206	-1.968914	1.781709	0.007222	0.267639
-34.810983	-2.062128	1.786714	0.007145	0.267542
-35.608285	-1.956310	1.791718	0.007293	0.267330
-36.488081	-1.791787	1.796723	0.007457	0.267354
-36.038088	-1.904357	1.801728	0.007373	0.267188
-36.920599	-1.772700	1.806733	0.007537	0.267031
-36.526496	-1.845210	1.811738	0.007464	0.267027
-36.624881	-1.852878	1.816742	0.007482	0.266888
-36.766102	-1.856155	1.821747	0.007509	0.266731
-36.826672	-1.842602	1.826752	0.007520	0.266745
-36.547186	-1.939756	1.831757	0.007468	0.266493
-36.427768	-1.981993	1.836762	0.007446	0.266382
-36.762466	-1.926624	1.841766	0.007508	0.266352
-37.007076	-1.932675	1.846771	0.007553	0.266077
-36.821685	-1.965334	1.851776	0.007519	0.266083
-37.062181	-1.952826	1.856781	0.007564	0.265913
-37.153553	-1.965766	1.861786	0.007581	0.265752
-36.842596	-2.023709	1.866790	0.007523	0.265745
-36.964055	-2.048145	1.871795	0.007545	0.265491
-37.523757	-1.944192	1.876800	0.007650	0.265503
-37.905958	-1.900433	1.881805	0.007721	0.265362
-37.851815	-1.945901	1.886810	0.007711	0.265168
-38.025523	-1.913498	1.891814	0.007743	0.265173
-38.277081	-1.917961	1.896819	0.007790	0.264898
-38.055083	-1.967588	1.901824	0.007749	0.264848
-38.244503	-1.946504	1.906829	0.007784	0.264775
-38.633264	-1.922171	1.911834	0.007856	0.264521
-39.194957	-1.816585	1.916838	0.007961	0.264540
-39.166817	-1.846546	1.921843	0.007955	0.264404
-39.345041	-1.841391	1.926848	0.007989	0.264254
-39.689378	-1.779128	1.931853	0.008053	0.264252
-38.701992	-1.998379	1.936858	0.007869	0.264035
-39.276880	-1.919388	1.941862	0.007976	0.263895
-39.601112	-1.860397	1.946867	0.008036	0.263895
-39.462979	-1.939001	1.951872	0.008011	0.263601
-40.006922	-1.840841	1.956877	0.008112	0.263597
-40.020766	-1.855781	1.961882	0.008114	0.263501
-39.904026	-1.918808	1.966886	0.008093	0.263272
-40.288851	-1.847421	1.971891	0.008164	0.263279
-40.181458	-1.897249	1.976896	0.008144	0.263113
-40.365954	-1.888839	1.981901	0.008179	0.262974
-40.323960	-1.893177	1.986906	0.008171	0.262992
-40.824600	-1.859777	1.991910	0.008264	0.262675
-41.135181	-1.808794	1.996915	0.008322	0.262644
-40.853123	-1.893564	2.001920	0.008269	0.262460

-41.048715	-1.886269	2.011917	0.008306	0.262304
-40.954210	-1.959331	2.021914	0.008288	0.261995
-41.336427	-1.911193	2.031910	0.008359	0.261877
-41.360028	-1.938194	2.041907	0.008364	0.261704
-41.122493	-2.014161	2.051904	0.008319	0.261523
-41.224795	-2.025561	2.061901	0.008338	0.261357
-41.188428	-2.052834	2.071898	0.008332	0.261243
-41.780326	-1.979813	2.081894	0.008442	0.261051
-41.476046	-2.037288	2.091891	0.008385	0.261039
-41.765099	-2.002819	2.101888	0.008439	0.260939
-42.175571	-1.965174	2.111885	0.008515	0.260733
-42.010408	-1.994626	2.121882	0.008484	0.260737
-42.131417	-1.973890	2.131878	0.008507	0.260730
-42.018803	-1.994166	2.141875	0.008486	0.260731
-42.208265	-1.958318	2.151872	0.008521	0.260739
-42.411598	-1.920365	2.161869	0.008559	0.260744
-42.136551	-1.971935	2.171866	0.008508	0.260736
-42.287663	-1.945269	2.181862	0.008536	0.260731
-42.418825	-1.919460	2.191859	0.008560	0.260742
-42.235965	-1.954053	2.201856	0.008526	0.260735
-42.138964	-1.971713	2.211853	0.008508	0.260735
-41.921057	-2.012024	2.221850	0.008468	0.260732
-41.800031	-2.000820	2.231846	0.008445	0.260916
-41.530200	-2.026615	2.241843	0.008395	0.261046
-41.799265	-1.975002	2.251840	0.008445	0.261061
-42.078990	-1.923524	2.261837	0.008497	0.261064
-41.773702	-1.963461	2.271834	0.008440	0.261151
-41.407067	-1.994370	2.281830	0.008372	0.261349
-41.068954	-2.057797	2.291827	0.008309	0.261339
-41.239712	-2.025789	2.301824	0.008340	0.261344
-40.855376	-2.045902	2.311821	0.008269	0.261620
-41.018284	-2.004661	2.321818	0.008299	0.261684
-41.132938	-1.982255	2.331814	0.008320	0.261693
-40.762335	-2.000099	2.341811	0.008251	0.261967
-41.231588	-1.911209	2.351808	0.008339	0.261987
-41.079271	-1.894287	2.361805	0.008310	0.262234
-40.459736	-1.995009	2.371802	0.008195	0.262300
-40.570971	-1.936578	2.381798	0.008216	0.262511
-40.648847	-1.901372	2.391795	0.008230	0.262627
-40.296165	-1.920792	2.401792	0.008164	0.262874
-39.927025	-1.972375	2.411789	0.008096	0.262960
-39.580291	-1.996425	2.421786	0.008031	0.263175
-39.677359	-1.966773	2.431782	0.008049	0.263241
-39.190787	-2.004477	2.441779	0.007959	0.263520
-39.954379	-1.846100	2.451776	0.008101	0.263628
-39.315680	-1.913491	2.461773	0.007982	0.263896
-38.947090	-1.953176	2.471770	0.007913	0.264046
-38.913403	-1.928869	2.481766	0.007907	0.264213
-38.494775	-1.963874	2.491763	0.007829	0.264439
-38.543172	-1.937366	2.501760	0.007838	0.264536
-38.019112	-1.977923	2.511757	0.007740	0.264835
-37.839414	-1.986522	2.521754	0.007707	0.264967
-37.843055	-1.952968	2.531750	0.007707	0.265147
-37.493719	-1.965210	2.541747	0.007642	0.265427
-37.316785	-1.978887	2.551744	0.007609	0.265528
-36.726421	-2.047425	2.561741	0.007499	0.265740
-36.835033	-1.997295	2.571738	0.007520	0.265906
-37.015601	-1.932942	2.581734	0.007553	0.266078
-36.794996	-1.918833	2.591731	0.007512	0.266373
-36.187546	-1.997372	2.601728	0.007399	0.266546
-35.816433	-2.036468	2.611725	0.007330	0.266701
-35.681478	-2.010123	2.621722	0.007305	0.266977
-35.436596	-2.027670	2.631718	0.007259	0.267124
-35.595286	-1.962432	2.641715	0.007289	0.267321
-35.319751	-1.958458	2.651712	0.007237	0.267614
-34.825244	-2.015267	2.661709	0.007145	0.267793
-34.619513	-2.020346	2.671706	0.007107	0.267968
-34.203095	-2.045190	2.681702	0.007029	0.268243
-33.825118	-2.090078	2.691699	0.006959	0.268372
-33.812212	-2.055821	2.701696	0.006956	0.268570
-33.420327	-2.076891	2.711693	0.006883	0.268840
-33.550169	-2.021907	2.721690	0.006908	0.269010
-33.088961	-2.066946	2.731686	0.006822	0.269219
-33.403843	-1.963030	2.741683	0.006880	0.269470
-32.952198	-2.006849	2.751680	0.006796	0.269676
-32.513533	-2.053651	2.761677	0.006714	0.269853
-32.366397	-2.024449	2.771674	0.006687	0.270153
-32.179963	-2.016602	2.781670	0.006652	0.270377
-32.281104	-1.962415	2.791667	0.006671	0.270569
-32.138614	-1.952094	2.801664	0.006645	0.270763
-31.525672	-2.008268	2.811661	0.006530	0.271058
-31.714087	-1.935172	2.821658	0.006565	0.271266
-31.155506	-1.998179	2.831654	0.006461	0.271472
-30.874626	-2.006778	2.841651	0.006409	0.271698
-30.543782	-2.014917	2.851648	0.006347	0.271976
-30.634275	-1.958216	2.861645	0.006364	0.272190
-30.489658	-1.941993	2.871642	0.006337	0.272416
-29.976486	-1.992990	2.881638	0.006242	0.272641
-29.979883	-1.932620	2.891635	0.006242	0.272958
-29.857391	-1.914088	2.901632	0.006219	0.273175
-30.017535	-1.834338	2.911629	0.006249	0.273443
-29.370565	-1.908689	2.921626	0.006129	0.273673
-28.880725	-1.954682	2.931622	0.006038	0.273901
-28.313982	-2.000050	2.941619	0.005932	0.274206
-28.168413	-1.989514	2.951616	0.005905	0.274401
-28.090074	-1.965054	2.961613	0.005890	0.274605
-27.649570	-1.999752	2.971610	0.005808	0.274845
-27.756481	-1.924066	2.981606	0.005828	0.275141
-27.515035	-1.920322	2.991603	0.005783	0.275392
-26.753846	-2.023279	3.001600	0.005641	0.275578
-26.841768	-1.974218	3.011597	0.005658	0.275752
-26.678326	-1.944079	3.021594	0.005627	0.276066
-26.548398	-1.926179	3.031590	0.005603	0.276284
-26.233639	-1.940511	3.041587	0.005544	0.276509
-25.901220	-1.956297	3.051584	0.005482	0.276743
-25.729401	-1.938081	3.061581	0.005450	0.277002
-25.841151	-1.862884	3.071578	0.005471	0.277289
-25.230801	-1.928745	3.081574	0.005358	0.277524
-24.929388	-1.941867	3.091571	0.005301	0.277742
-24.446559	-1.985056	3.101568	0.005212	0.277974
-24.303073	-1.956592	3.111565	0.005185	0.278258
-24.375174	-1.898051	3.121562	0.005198	0.278495
-24.148594	-1.893472	3.131558	0.005156	0.278733
-23.713451	-1.930998	3.141555	0.005075	0.278949
-23.598542	-1.898723	3.151552	0.005053	0.279225
-23.344816	-1.890173	3.161549	0.005006	0.279508
-23.289140	-1.852665	3.171546	0.004996	0.279755
-23.265135	-1.806888	3.181542	0.004991	0.280015
-22.589341	-1.882005	3.191539	0.004865	0.280261
-22.079416	-1.928149	3.201536	0.004770	0.280502
-22.201876	-1.859224	3.211533	0.004793	0.280743
-21.882089	-1.870144	3.221530	0.004734	0.280986
-22.071122	-1.786449	3.231526	0.004769	0.281241
-21.661449	-1.808424	3.241523	0.004692	0.281511
-21.309147	-1.822193	3.251520	0.004627	0.281769
-20.816970	-1.867991	3.261517	0.004535	0.281994
-20.439756	-1.878460	3.271514	0.004465	0.282292
-20.370738	-1.846839	3.281510	0.004452	0.282519
-20.409882	-1.788226	3.291507	0.004459	0.282783
-20.028476	-1.807717	3.301504	0.004388	0.283038
-19.367348	-1.885733	3.311501	0.004265	0.283254
-19.092506	-1.875810	3.321498	0.004214	0.283560
-19.694226	-1.717089	3.331494	0.004326	0.283812
-18.906210	-1.808487	3.341491	0.004179	0.284076
-18.453699	-1.847447	3.351488	0.004095	0.284297
-18.328896	-1.825767	3.361485	0.004072	0.284523
-17.924003	-1.838633	3.371482	0.003996	0.284832
-17.557103	-1.861933	3.381478	0.003928	0.285052
-17.370431	-1.851774	3.391475	0.003893	0.285276
-16.979978	-1.877785	3.401472	0.003820	0.285505
-16.659005	-1.889449	3.411469	0.003761	0.285741
-16.348930	-1.901254	3.421466	0.003703	0.285967
-16.154499	-1.897129	3.431462	0.003667	0.286167
-15.849493	-1.913898	3.441459	0.003610	0.286363
-15.588484	-1.896085	3.451456	0.003561	0.286692
-15.002507	-1.969407	3.461453	0.003452	0.286860
-14.837516	-1.964722	3.471450	0.003421	0.287035
-14.545774	-1.965333	3.481446	0.003367	0.287300
-14.040650	-2.012424	3.491443	0.003273	0.287525
-14.111526	-1.963825	3.501440	0.003286	0.287705
-14.043329	-1.922309	3.511437	0.003273	0.287976
-13.577058	-1.959159	3.521434	0.003186	0.288217
-13.531509	-1.929525	3.531430	0.003178	0.288407
-13.368013	-1.919427	3.541427	0.003147	0.288607
-12.988921	-1.934480	3.551424	0.003077	0.288877
-12.644506	-1.947116	3.561421	0.003013	0.289128
-12.610103	-1.913660	3.571418	0.003006	0.289327
-12.088464	-1.973811	3.581414	0.002909	0.289500
-11.901296	-1.945222	3.591411	0.002874	0.289813
-11.595487	-1.963667	3.601408	0.002817	0.289999
-11.313864	-1.977208	3.611405	0.002765	0.290187
-11.207654	-1.934725	3.621402	0.002745	0.290495
-10.942037	-1.947054	3.631398	0.002696	0.290674
-10.908870	-1.916520	3.641395	0.002689	0.290856
-10.235976	-1.998724	3.651392	0.002564	0.291056
-9.843315	-2.012958	3.661389	0.002491	0.291340
-9.921329	-1.960685	3.671386	0.002505	0.291529
-9.505890	-1.999806	3.681382	0.002428	0.291710
-9.709023	-1.905648	3.691379	0.002466	0.291994
-9.621844	-1.873431	3.701376	0.002450	0.292232
-9.404974	-1.866731	3.711373	0.002409	0.292460
-8.999689	-1.895990	3.721370	0.002334	0.292680
-8.884196	-1.856137	3.731366	0.002312	0.292981
-8.805783	-1.820789	3.741363	0.002297	0.293226
-8.575360	-1.814342	3.751360	0.002254	0.293465
-8.182428	-1.840272	3.761357	0.002181	0.293689
-7.831771	-1.860216	3.771354	0.002116	0.293905
-7.584502	-1.838160	3.781350	0.002070	0.294235
-7.534730	-1.804993	3.791347	0.002061	0.294442
-7.161195	-1.827604	3.801344	0.001991	0.294665
-6.991411	-1.809886	3.811341	0.001959	0.294904
-6.641263	-1.818942	3.821338	0.001894	0.295171
-6.476048	-1.786627	3.831334	0.001863	0.295477
-6.514304	-1.739201	3.841331	0.001870	0.295675
-6.257551	-1.739207	3.851328	0.001823	0.295904
-6.147844	-1.707508	3.861325	0.001802	0.296156
-5.842418	-1.713063	3.871322	0.001745	0.296400
-5.678503	-1.677349	3.881318	0.001715	0.296720
-5.237169	-1.708230	3.891315	0.001632	0.296961
-5.390918	-1.623145	3.901312	0.001661	0.297239
-4.694455	-1.700616	3.911309	0.001531	0.297478
-5.163038	-1.553825	3.921306	0.001619	0.297778
-5.060382	-1.512342	3.931302	0.001599	0.298070
-4.621627	-1.539203	3.941299	0.001518	0.298327
-4.298370	-1.540760	3.951296	0.001457	0.298604
-4.086527	-1.517120	3.961293	0.001418	0.298905
-3.634083	-1.535249	3.971290	0.001334	0.299216
-3.353543	-1.535627	3.981286	0.001281	0.299460
-3.089308	-1.528889	3.991283	0.001232	0.299725
-3.098793	-1.468800	4.001280	0.001234	0.300007
-2.862641	-1.452060	4.011277	0.001190	0.300294
-2.969754	-1.371387	4.021274	0.001210	0.300589
-3.217803	-1.269603	4.031270	0.001256	0.300862
-2.459323	-1.347289	4.041267	0.001115	0.301152
-2.255593	-1.322470	4.051264	0.001077	0.301449
-2.077361	-1.288770	4.061261	0.001043	0.301766
-1.781430	-1.285444	4.071258	0.000988	0.302040
-1.383801	-1.293937	4.081254	0.000914	0.302345
-1.607047	-1.186726	4.091251	0.000956	0.302664
-1.927782	-1.050986	4.101248	0.001015	0.303034
-1.569837	-1.049881	4.111245	0.000949	0.303350
-1.167254	-1.055632	4.121242	0.000874	0.303671
-1.497461	-0.920220	4.131238	0.000935	0.304031
-1.885127	-0.771160	4.141235	0.001007	0.304405
-1.989659	-0.671753	4.151232	0.001026	0.304787
-1.542224	-0.669577	4.161229	0.000943	0.305183
-1.810445	-0.527511	4.171226	0.000993	0.305625
-1.240013	-0.562703	4.181222	0.000887	0.305949
-1.344477	-0.462325	4.191219	0.000906	0.306334
-1.117953	-0.411673	4.201216	0.000864	0.306767
-0.784509	-0.390620	4.211213	0.000802	0.307152
-0.597495	-0.341426	4.221210	0.000767	0.307544
-0.000546	-0.365318	4.231206	0.000656	0.307942
-0.491493	-0.180943	4.241203	0.000747	0.308389
-0.284725	-0.134980	4.251200	0.000708	0.308781
0.197704	-0.135913	4.261197	0.000619	0.309187
0.104676	-0.023728	4.271194	0.000636	0.309632
0.144293	0.059068	4.281190	0.000628	0.310053
-0.101401	0.206694	4.291187	0.000674	0.310533
0.000000	0.273581	4.301184	0.000655	0.310930

0.077312	0.532375	4.306189	0.000640	0.312197
0.438552	1.033294	4.311194	0.000573	0.314812
0.571506	1.856185	4.316198	0.000547	0.318681
0.637643	2.981741	4.321203	0.000534	0.323805
1.282138	4.295215	4.326208	0.000414	0.330135
1.294718	6.019853	4.331213	0.000410	0.337618
1.763900	7.964318	4.336218	0.000321	0.346206
1.909617	10.273666	4.341222	0.000293	0.355833
2.742173	12.759677	4.346227	0.000136	0.366398
2.977773	15.687374	4.351232	0.000090	0.377945
3.144797	18.950755	4.356237	0.000057	0.390349
4.188137	22.384230	4.361242	-0.000139	0.403552
4.895415	26.229895	4.366246	-0.000274	0.417554
5.720200	30.401059	4.371251	-0.000430	0.432263
6.753935	34.881232	4.376256	-0.000625	0.447610
7.378204	39.789960	4.381261	-0.000745	0.463555
8.377837	44.980615	4.386266	-0.000934	0.480023
9.133595	50.563167	4.391270	-0.001079	0.496958
12.505207	56.032426	4.396275	-0.001710	0.514343
17.168395	61.636931	4.401280	-0.002582	0.532157
18.654950	68.163769	4.406285	-0.002863	0.550312
19.725983	75.088623	4.411290	-0.003067	0.568708
21.079220	82.267361	4.416294	-0.003324	0.587278
23.150553	89.610590	4.421299	-0.003714	0.605977
26.170753	97.076728	4.426304	-0.004281	0.624792
27.374270	105.130161	4.431309	-0.004511	0.643644
28.594145	113.429447	4.436314	-0.004743	0.662501
29.595864	121.956049	4.441318	-0.004935	0.681234
31.318347	130.570018	4.446323	-0.005262	0.699912
32.972441	139.368466	4.451328	-0.005576	0.718449
34.570564	148.338965	4.456333	-0.005879	0.736836
36.730563	157.366945	4.461338	-0.006287	0.755076
38.532771	166.571305	4.466342	-0.006629	0.773094
39.844011	175.980733	4.471347	-0.006879	0.790916
42.592066	185.188099	4.476352	-0.007397	0.808437
44.295188	194.705897	4.481357	-0.007720	0.825805
45.354179	204.390068	4.486362	-0.007923	0.842903
46.410613	214.065665	4.491366	-0.008127	0.859646
47.328586	223.798324	4.496371	-0.008304	0.876121
49.603634	233.296306	4.501376	-0.008734	0.892298
52.120486	242.762853	4.506381	-0.009208	0.908203
53.691796	252.404564	4.511386	-0.009507	0.923847
55.621201	261.970826	4.516390	-0.009873	0.939209
56.678074	271.685529	4.521395	-0.010076	0.954317
57.988074	281.303285	4.526400	-0.010326	0.969109
60.449076	290.695344	4.531405	-0.010791	0.983642
62.735495	300.116577	4.536410	-0.011222	0.997960
63.867158	309.657199	4.541414	-0.011439	1.011957
64.655345	319.228601	4.546419	-0.011592	1.025721
66.270334	328.589815	4.551424	-0.011899	1.039210
68.457352	337.802911	4.556429	-0.012312	1.052458
70.507622	347.039897	4.561434	-0.012700	1.065540
71.420701	356.394736	4.566438	-0.012876	1.078357
72.645789	365.624176	4.571443	-0.013110	1.090928
73.000889	374.984915	4.576448	-0.013183	1.103331
74.558307	384.043009	4.581453	-0.013479	1.115472
75.924161	393.105303	4.586458	-0.013739	1.127444
76.839604	402.205815	4.591462	-0.013915	1.139240
78.703795	411.098181	4.596467	-0.014268	1.150857
80.182118	420.012638	4.601472	-0.014549	1.162303
80.747944	429.044028	4.606477	-0.014661	1.173588
81.496635	438.002452	4.611482	-0.014806	1.184715
82.678728	446.815449	4.616486	-0.015032	1.195651
84.129403	455.564245	4.621491	-0.015307	1.206465
85.616599	464.284704	4.626496	-0.015590	1.217157
85.794101	473.190641	4.631501	-0.015629	1.227710
87.055716	481.866207	4.636506	-0.015870	1.238120
87.341436	490.669123	4.641510	-0.015928	1.248398
88.331323	499.308980	4.646515	-0.016118	1.258542
90.384338	507.758093	4.651520	-0.016506	1.268592
92.870797	516.134286	4.656525	-0.016975	1.278562
93.744937	524.802980	4.661530	-0.017143	1.288477
93.590588	533.604849	4.666534	-0.017120	1.298271
95.187436	542.080376	4.671539	-0.017423	1.307957
96.316316	550.653539	4.676544	-0.017639	1.317591
97.061977	559.169285	4.681549	-0.017783	1.327023
97.960995	567.687466	4.686554	-0.017956	1.336418
97.898097	576.338028	4.691558	-0.017950	1.345717
98.948545	584.757731	4.696563	-0.018151	1.354904
101.775619	592.872904	4.701568	-0.018683	1.364020
102.761070	601.339095	4.706573	-0.018872	1.373121
103.860122	609.762848	4.711578	-0.019082	1.382137
104.683877	618.214252	4.716582	-0.019241	1.391075
106.674104	626.454591	4.721587	-0.019617	1.399938
107.548970	634.917741	4.726592	-0.019785	1.408783
109.132055	643.208624	4.731597	-0.020086	1.417517
110.861445	651.473583	4.736602	-0.020413	1.426194
110.933543	660.042901	4.741606	-0.020432	1.434849
111.684213	668.420656	4.746611	-0.020577	1.443373
113.351764	676.682823	4.751616	-0.020893	1.451881
114.091930	685.079069	4.756621	-0.021036	1.460321
115.347802	693.385834	4.761626	-0.021276	1.468708
115.203544	701.931925	4.766630	-0.021254	1.477055
115.990642	710.231228	4.771635	-0.021406	1.485264
116.436535	718.614259	4.776640	-0.021495	1.493455
117.398362	726.844673	4.781645	-0.021679	1.501535
118.936795	735.041367	4.786650	-0.021971	1.509630
120.777477	743.180253	4.791654	-0.022319	1.517673
122.405112	751.364811	4.796659	-0.022628	1.525683
123.223980	759.728388	4.801664	-0.022786	1.533695
123.685147	768.077532	4.806669	-0.022877	1.541597
124.258741	776.423902	4.811674	-0.022989	1.549473
125.116093	784.687094	4.816678	-0.023154	1.557274
125.787346	792.964729	4.821683	-0.023285	1.565022
126.401101	801.285234	4.826688	-0.023404	1.572763
126.993056	809.542954	4.831693	-0.023520	1.580404
127.614238	817.837211	4.836698	-0.023641	1.588046
128.310115	826.063292	4.841702	-0.023776	1.595601
129.256097	834.250964	4.846707	-0.023957	1.603121
130.163537	842.462652	4.851712	-0.024132	1.610622
130.782798	850.733043	4.856717	-0.024252	1.618098
131.688441	858.941621	4.861722	-0.024426	1.625526
132.850864	867.124721	4.866726	-0.024648	1.632934
133.524289	875.350554	4.871731	-0.024779	1.640277
134.881918	883.461911	4.876736	-0.025037	1.647582
135.930431	891.637600	4.881741	-0.025238	1.654868
136.852755	899.862913	4.886746	-0.025415	1.662146
137.839253	908.047002	4.891750	-0.025604	1.669366
138.683674	916.254485	4.896755	-0.025766	1.676555
139.289023	924.487824	4.901760	-0.025885	1.683703
139.938670	932.703512	4.906765	-0.026011	1.690812
141.188678	940.866597	4.911770	-0.026249	1.697926
141.237670	949.184961	4.916774	-0.026263	1.704981
142.080864	957.353824	4.921779	-0.026426	1.711987
142.595264	965.561313	4.926784	-0.026527	1.718952
143.019462	973.758210	4.931789	-0.026611	1.725869
143.543023	981.986906	4.936794	-0.026714	1.732797
144.612208	990.086872	4.941798	-0.026919	1.739662
145.213192	998.287421	4.946803	-0.027036	1.746522
145.663545	1006.530245	4.951808	-0.027125	1.753370
146.988856	1014.559947	4.956813	-0.027377	1.760130
147.232822	1022.824290	4.961818	-0.027428	1.766916
148.058653	1030.968729	4.966822	-0.027587	1.773653
148.899564	1039.108515	4.971827	-0.027749	1.780362
150.131043	1047.228901	4.976832	-0.027983	1.787079
150.560733	1055.458248	4.981837	-0.028069	1.793757
151.151529	1063.624276	4.986842	-0.028184	1.800380
152.080998	1071.728113	4.991846	-0.028363	1.806971
153.071382	1079.857353	4.996851	-0.028552	1.813566
153.725400	1088.014238	5.001856	-0.028679	1.820117
154.031413	1096.234789	5.006861	-0.028742	1.826652
154.835442	1104.387965	5.011866	-0.028897	1.833171
155.399214	1112.539062	5.016870	-0.029007	1.839636
155.937085	1120.702590	5.021875	-0.029113	1.846085
156.744092	1128.835952	5.026880	-0.029268	1.852520
157.398482	1136.961614	5.031885	-0.029395	1.858908
158.193062	1145.071126	5.036890	-0.029549	1.865278
158.956955	1153.232075	5.041894	-0.029696	1.871663
159.551692	1161.376099	5.046899	-0.029812	1.877992
159.706306	1169.577454	5.051904	-0.029846	1.884293
160.053320	1177.745326	5.056909	-0.029916	1.890569
160.507436	1185.908540	5.061914	-0.030006	1.896833
161.006011	1194.015514	5.066918	-0.030104	1.903039
161.884563	1202.082154	5.071923	-0.030273	1.909238
162.502392	1210.230342	5.076928	-0.030394	1.915448
163.114543	1218.339377	5.081933	-0.030513	1.921608
163.766942	1226.483528	5.086938	-0.030640	1.927779
164.299880	1234.619221	5.091942	-0.030744	1.933910
164.822367	1242.754221	5.096947	-0.030847	1.940020
164.731855	1251.004632	5.101952	-0.030835	1.946128
165.528646	1259.062880	5.106957	-0.030989	1.952173
166.500376	1267.102260	5.111962	-0.031175	1.958205
166.739835	1275.228339	5.116966	-0.031225	1.964201
168.030952	1283.218296	5.121971	-0.031471	1.970194
168.651640	1291.380618	5.126976	-0.031592	1.976222
169.653986	1299.438072	5.131981	-0.031783	1.982196
169.856929	1307.671178	5.136986	-0.031827	1.988192
171.016794	1315.686932	5.141990	-0.032048	1.994117
172.465004	1323.663532	5.146995	-0.032323	2.000026
173.129714	1331.830690	5.152000	-0.032452	2.005971
173.604340	1339.987463	5.157005	-0.032545	2.011870
174.180492	1348.171897	5.162010	-0.032658	2.017783
174.778162	1356.263832	5.167014	-0.032775	2.023614
175.706307	1364.338183	5.172019	-0.032953	2.029451
176.178396	1372.508614	5.177024	-0.033046	2.035291
176.637559	1380.614578	5.182029	-0.033137	2.041067
177.209909	1388.739858	5.187034	-0.033249	2.046853
177.873868	1396.844872	5.192038	-0.033378	2.052617
178.625957	1404.935061	5.197043	-0.033523	2.058363
178.947879	1413.082341	5.202048	-0.033588	2.064089
179.086021	1421.237074	5.207053	-0.033619	2.069785
180.051021	1429.283198	5.212058	-0.033804	2.075475
180.603991	1437.380414	5.217062	-0.033912	2.081142
180.837207	1445.523561	5.222067	-0.033961	2.086793
181.137915	1453.680503	5.227072	-0.034022	2.092445
181.184636	1461.827844	5.232077	-0.034037	2.098050
181.790197	1469.888611	5.237082	-0.034155	2.103636
182.248566	1477.996791	5.242086	-0.034245	2.109225
182.634318	1486.125926	5.247091	-0.034322	2.114806
183.469583	1494.134974	5.252096	-0.034483	2.120335
183.754321	1502.228868	5.257101	-0.034541	2.125853
184.772286	1510.266062	5.262106	-0.034736	2.131390
185.228190	1518.367359	5.267110	-0.034826	2.136901
185.497885	1526.488895	5.272115	-0.034882	2.142393
186.238456	1534.561421	5.277120	-0.035025	2.147884
186.688618	1542.641586	5.282125	-0.035114	2.153337
187.199412	1550.741851	5.287130	-0.035215	2.158796
187.566870	1558.843440	5.292134	-0.035288	2.164228
188.480718	1566.870801	5.297139	-0.035464	2.169649
189.222856	1574.955976	5.302144	-0.035607	2.175078
189.680719	1583.062775	5.307149	-0.035698	2.180482
190.481116	1591.138630	5.312154	-0.035852	2.185883
191.352217	1599.201021	5.317158	-0.036019	2.191269
192.107439	1607.271799	5.322163	-0.036165	2.196635
192.911653	1615.331113	5.327168	-0.036320	2.201986
193.074823	1623.479452	5.332173	-0.036356	2.207322
193.121568	1631.661480	5.337178	-0.036370	2.212657
193.600712	1639.728380	5.342182	-0.036465	2.217944
194.463331	1647.732822	5.347187	-0.036630	2.223212
195.606909	1655.772402	5.352192	-0.036849	2.228516
196.173402	1663.875884	5.357197	-0.036959	2.233796
196.925562	1671.953458	5.362202	-0.037105	2.239064
197.612777	1680.012029	5.367206	-0.037238	2.244301
198.120249	1688.121704	5.372211	-0.037338	2.249542
198.534227	1696.255685	5.377216	-0.037420	2.254778
198.859447	1704.347765	5.382221	-0.037486	2.259967
199.333001	1712.447577	5.387226	-0.037579	2.265163
199.831006	1720.548897	5.392230	-0.037677	2.270349
200.205805	1728.656394	5.397235	-0.037753	2.275517
200.864776	1736.689454	5.402240	-0.037881	2.280650
201.127499	1744.759374	5.407245	-0.037935	2.285761
201.611236	1752.835322	5.412250	-0.038030	2.290883
201.845806	1760.947235	5.417254	-0.038079	2.295995
202.341862	1768.991621	5.422259	-0.038177	2.301075
202.820291	1777.079586	5.427264	-0.038271	2.306170
203.715500	1785.091782	5.432269	-0.038443	2.311242
204.607973	1793.103247	5.437274	-0.038614	2.316302
205.112485	1801.175826	5.442278	-0.038714	2.321355
205.433010	1809.288061	5.447283	-0.038779	2.326407
205.910387	1817.399716	5.452288	-0.038873	2.331460
206.039780	1825.512785	5.457293	-0.038902	2.336474
206.132134	1833.646664	5.462298	-0.038925	2.341486
207.004637	1841.622696	5.467302	-0.039092	2.346457
207.670183	1849.678350	5.472307	-0.039222	2.351448
208.477019	1857.710907	5.477312	-0.039377	2.356426
208.822924	1865.787732	5.482317	-0.039447	2.361382
209.254105	1873.894340	5.487322	-0.039532	2.366353
210.027811	1881.931033	5.492326	-0.039682	2.371299
210.489746	1890.023576	5.497331	-0.039773	2.376243
210.773164	1898.135180	5.502336	-0.039831	2.381173
210.901667	1906.232912	5.507341	-0.039860	2.386073
211.875324	1914.245831	5.512346	-0.040047	2.390979
212.485346	1922.289136	5.517350	-0.040166	2.395864
213.357951	1930.281225	5.522355	-0.040333	2.400730
213.743190	1938.396135	5.527360	-0.040410	2.405620
214.521577	1946.431815	5.532365	-0.040560	2.410484
215.318522	1954.490685	5.537370	-0.040714	2.415353
215.780243	1962.576944	5.542374	-0.040805	2.420202
215.712771	1970.734177	5.547379	-0.040798	2.425041
216.945761	1978.737078	5.552384	-0.041033	2.429882
217.246627	1986.859952	5.557389	-0.041094	2.434711
217.644669	1994.928576	5.562394	-0.041174	2.439505
218.289225	2002.936946	5.567398	-0.041299	2.444274
218.631347	2011.042825	5.572403	-0.041368	2.449067
219.345849	2019.086106	5.577408	-0.041506	2.453843
219.972510	2027.109896	5.582413	-0.041628	2.458591
220.601353	2035.157880	5.587418	-0.041750	2.463345
220.765719	2043.282603	5.592422	-0.041786	2.468098
221.343927	2051.306281	5.597427	-0.041899	2.472814
222.223985	2059.339444	5.602432	-0.042068	2.477551
222.385184	2067.440859	5.607437	-0.042104	2.482262
222.715743	2075.538356	5.612442	-0.042171	2.486976
223.246113	2083.591847	5.617446	-0.042275	2.491670
223.605490	2091.681792	5.622451	-0.042347	2.496363
224.650455	2099.643492	5.627456	-0.042547	2.501025
224.852239	2107.743805	5.632461	-0.042589	2.505695
225.406643	2115.831901	5.637466	-0.042698	2.510375
225.450877	2123.960013	5.642470	-0.042711	2.515032
226.275701	2131.920847	5.647475	-0.042870	2.519642
227.405940	2139.867780	5.652480	-0.043086	2.524257
227.882707	2147.974295	5.657485	-0.043180	2.528908
228.137409	2156.097669	5.662490	-0.043233	2.533542
228.871969	2164.121278	5.667494	-0.043375	2.538147
229.360044	2172.178024	5.672499	-0.043471	2.542744
230.206709	2180.208163	5.677504	-0.043634	2.547343
230.434581	2188.310050	5.682509	-0.043681	2.551930
231.146355	2196.369321	5.687514	-0.043819	2.556520
231.294547	2204.474236	5.692518	-0.043852	2.561086
231.760835	2212.528166	5.697523	-0.043944	2.565638
232.576123	2220.571035	5.702528	-0.044101	2.570201
233.402268	2228.543496	5.707533	-0.044260	2.574716
233.647484	2236.682460	5.712538	-0.044311	2.579276
234.212690	2244.715861	5.717542	-0.044422	2.583791
234.673286	2252.786717	5.722547	-0.044513	2.588312
235.642169	2260.861072	5.727552	-0.044699	2.592862
235.908179	2268.942572	5.732557	-0.044753	2.597359
236.083819	2277.019956	5.737562	-0.044791	2.601840
236.103858	2285.122138	5.742566	-0.044800	2.606315
237.159886	2293.021722	5.747571	-0.045002	2.610743
237.713183	2301.104440	5.752576	-0.045110	2.615229
237.357811	2309.256031	5.757581	-0.045050	2.619683
237.976042	2317.244592	5.762586	-0.045170	2.624107
238.436756	2325.288887	5.767590	-0.045261	2.628543
239.108961	2333.283605	5.772595	-0.045391	2.632959
239.448985	2341.378916	5.777600	-0.045460	2.637399
239.672315	2349.431136	5.782605	-0.045507	2.641801
241.078685	2357.333008	5.787610	-0.045774	2.646193
241.843769	2365.393123	5.792614	-0.045922	2.650620
242.224820	2373.488324	5.797619	-0.045998	2.655033
242.572290	2381.597035	5.802624	-0.046068	2.659444
243.175210	2389.626126	5.807629	-0.046185	2.663821
243.828199	2397.676551	5.812634	-0.046312	2.668206
244.337509	2405.744298	5.817638	-0.046412	2.672583
244.776085	2413.773785	5.822643	-0.046499	2.676928
245.465279	2421.794702	5.827648	-0.046633	2.681278
245.475545	2429.897288	5.832653	-0.046640	2.685620
246.645464	2437.870035	5.837658	-0.046863	2.689961
246.369170	2446.055587	5.842662	-0.046817	2.694314
246.561066	2454.129416	5.847667	-0.046858	2.698631
247.125005	2462.165339	5.852672	-0.046968	2.702945
247.485665	2470.195528	5.857677	-0.047041	2.707236
247.714450	2478.298770	5.862682	-0.047088	2.711550
248.488939	2486.269040	5.867686	-0.047238	2.715822
249.555793	2494.197032	5.872691	-0.047442	2.720083
250.077363	2502.242087	5.877696	-0.047544	2.724365
250.673962	2510.295847	5.882701	-0.047660	2.728649
250.994294	2518.440829	5.887706	-0.047725	2.732956
251.511355	2526.479615	5.892710	-0.047827	2.737214
251.799250	2534.535964	5.897715	-0.047886	2.741460
251.820200	2542.662443	5.902720	-0.047895	2.745719
252.650442	2550.654471	5.907725	-0.048055	2.749951
253.170892	2558.727814	5.912730	-0.048157	2.754200
253.310443	2566.801601	5.917734	-0.048188	2.758419
253.535859	2574.826666	5.922739	-0.048235	2.762612
254.507508	2582.792053	5.927744	-0.048422	2.766813
254.828753	2590.855911	5.932749	-0.048487	2.771018
255.372888	2598.913783	5.937754	-0.048593	2.775228
255.979484	2606.918300	5.942758	-0.048711	2.779407
256.397375	2614.944685	5.947763	-0.048794	2.783580
257.086630	2623.007858	5.952768	-0.048928	2.787782
257.655678	2631.036416	5.957773	-0.049039	2.791953
257.451443	2639.210796	5.962778	-0.049007	2.796145
258.264076	2647.166174	5.967782	-0.049163	2.800280
258.373567	2655.220542	5.972787	-0.049189	2.804417
258.823676	2663.293638	5.977792	-0.049278	2.808578
259.090096	2671.347743	5.982797	-0.049333	2.812712
259.579632	2679.391061	5.987802	-0.049429	2.816848
260.313792	2687.364258	5.992806	-0.049571	2.820956
260.047764	2695.498757	5.997811	-0.049527	2.825082
260.745042	2703.492769	6.002816	-0.049662	2.829186
261.288053	2711.527621	6.007821	-0.049768	2.833296
261.757898	2719.553272	6.012826	-0.049861	2.837392
262.202706	2727.583781	6.017830	-0.049949	2.841482
262.517372	2735.626182	6.022835	-0.050013	2.845564
262.885627	2743.702050	6.027840	-0.050087	2.849661
263.016960	2751.773387	6.032845	-0.050116	2.853736
262.748637	2759.927325	6.037850	-0.050072	2.857823
263.663605	2767.851912	6.042854	-0.050247	2.861858
263.932104	2775.880885	6.047859	-0.050303	2.865902
264.447435	2783.942016	6.052864	-0.050404	2.869970
264.321810	2792.029944	6.057869	-0.050386	2.874009
264.559419	2800.081914	6.062874	-0.050435	2.878046
264.724675	2808.102137	6.067878	-0.050471	2.882057
265.515088	2816.043834	6.072883	-0.050624	2.886058
266.065440	2824.114385	6.077888	-0.050731	2.890104
265.937295	2832.211027	6.082893	-0.050713	2.894120
266.792243	2840.172896	6.087898	-0.050877	2.898117
267.470464	2848.200036	6.092902	-0.051009	2.902132
267.988219	2856.235102	6.097907	-0.051110	2.906136
267.972252	2864.414961	6.102912	-0.051113	2.910176
267.622961	2872.588153	6.107917	-0.051053	2.914190
268.287145	2880.509051	6.112922	-0.051182	2.918129
269.268121	2888.421797	6.117926	-0.051370	2.922076
269.639731	2896.437323	6.122931	-0.051444	2.926034
270.666006	2904.417117	6.127936	-0.051640	2.930005
270.956230	2912.496417	6.132941	-0.051700	2.933980
270.983086	2920.597293	6.137946	-0.051710	2.937946
271.377649	2928.611866	6.142950	-0.051789	2.941883
271.933400	2936.592204	6.147955	-0.051897	2.945808
272.469780	2944.665096	6.152960	-0.052003	2.949771
272.894246	2952.721567	6.157965	-0.052087	2.953715
273.353356	2960.782695	6.162970	-0.052178	2.957657
273.822908	2968.802208	6.167974	-0.052270	2.961574
274.581711	2976.808271	6.172979	-0.052417	2.965495
274.999438	2984.888782	6.177984	-0.052500	2.969429
275.728777	2992.884483	6.182989	-0.052641	2.973333
275.976963	3000.976066	6.187994	-0.052692	2.977253
276.415735	3009.031985	6.192998	-0.052779	2.981160
276.863509	3017.023787	6.198003	-0.052868	2.985031
277.437942	3025.085359	6.203008	-0.052980	2.988938
277.581548	3033.153257	6.208013	-0.053012	2.992820
277.917527	3041.199398	6.213018	-0.053080	2.996697
278.063550	3049.265353	6.218022	-0.053112	3.000568
278.662816	3057.200745	6.223027	-0.053229	3.004395
278.950099	3065.274596	6.228032	-0.053288	3.008267
279.269855	3073.322170	6.233037	-0.053353	3.012123
279.657666	3081.357282	6.238042	-0.053430	3.015972
279.957814	3089.423310	6.243046	-0.053491	3.019826
280.104610	3097.470664	6.248051	-0.053524	3.023659
281.070365	3105.420876	6.253056	-0.053709	3.027482
281.447376	3113.495026	6.258061	-0.053784	3.031328
282.164288	3121.508296	6.263066	-0.053923	3.035159
282.384339	3129.576919	6.268070	-0.053969	3.038985
282.942075	3137.566246	6.273075	-0.054079	3.042786
283.340305	3145.656039	6.278080	-0.054158	3.046622
283.886911	3153.666502	6.283085	-0.054265	3.050423
283.990596	3161.747962	6.288090	-0.054290	3.054230
284.716411	3169.747673	6.293094	-0.054430	3.058025
284.675358	3177.819264	6.298099	-0.054428	3.061811
285.332338	3185.829911	6.303104	-0.054555	3.065598
285.654221	3193.868752	6.308109	-0.054620	3.069378
286.459309	3201.906597	6.313114	-0.054775	3.073175
286.846534	3209.936945	6.318118	-0.054853	3.076944
286.972750	3218.018224	6.323123	-0.054882	3.080719
287.415658	3226.022702	6.328128	-0.054969	3.084469
287.706970	3234.053343	6.333133	-0.055029	3.088220
288.213742	3242.097441	6.338138	-0.055128	3.091982
289.200292	3250.056932	6.343142	-0.055317	3.095723
289.778919	3258.035725	6.348147	-0.055430	3.099449
290.149556	3266.104915	6.353152	-0.055505	3.103203
290.230832	3274.218805	6.358157	-0.055525	3.106959
290.465424	3282.287151	6.363162	-0.055574	3.110697
290.945857	3290.281599	6.368166	-0.055669	3.114407
291.746936	3298.222339	6.373171	-0.055823	3.118103
292.282623	3306.291240	6.378176	-0.055928	3.121842
292.577244	3314.319536	6.383181	-0.055988	3.125546
293.052747	3322.367970	6.388186	-0.056082	3.129263
293.540080	3330.412099	6.393190	-0.056178	3.132974
293.837095	3338.482283	6.398195	-0.056238	3.136684
294.077390	3346.552806	6.403200	-0.056288	3.140387
294.751829	3354.500279	6.408205	-0.056419	3.144049
295.059958	3362.576520	6.413210	-0.056482	3.147749
295.444438	3370.657611	6.418214	-0.056559	3.151450
295.586558	3378.700996	6.423219	-0.056590	3.155118
296.387218	3386.671718	6.428224	-0.056745	3.158779
296.496585	3394.716686	6.433229	-0.056770	3.162439
296.927084	3402.756020	6.438234	-0.056856	3.166105
297.307740	3410.791863	6.443238	-0.056932	3.169764
297.400715	3418.849457	6.448243	-0.056954	3.173415
298.040293	3426.861645	6.453248	-0.057079	3.177066
297.721519	3434.983661	6.458253	-0.057025	3.180720
298.272770	3442.902163	6.463258	-0.057133	3.184317
298.860373	3450.958787	6.468262	-0.057247	3.187972
299.288750	3458.968197	6.473267	-0.057332	3.191596
299.600123	3467.023254	6.478272	-0.057395	3.195230
299.998671	3475.022193	6.483277	-0.057475	3.198840
300.244537	3483.065265	6.488282	-0.057526	3.202458
300.568264	3491.168654	6.493286	-0.057592	3.206102
301.288070	3499.096177	6.498291	-0.057731	3.209680
302.088791	3507.146772	6.503296	-0.057885	3.213313
302.384466	3515.203324	6.508301	-0.057945	3.216923
303.010734	3523.193459	6.513306	-0.058067	3.220513
303.224407	3531.250284	6.518310	-0.058112	3.224111
303.022636	3539.371784	6.523315	-0.058080	3.227716
303.773057	3547.369953	6.528320	-0.058225	3.231303
304.635830	3555.304155	6.533325	-0.058391	3.234862
304.550094	3563.379922	6.538330	-0.058380	3.238439
304.936874	3571.410256	6.543334	-0.058457	3.242013
305.236344	3579.452903	6.548339	-0.058518	3.245584
305.493638	3587.516998	6.553344	-0.058572	3.249159
305.949597	3595.512810	6.558349	-0.058662	3.252708
306.711486	3603.505333	6.563354	-0.058809	3.256264
307.051623	3611.568226	6.568358	-0.058877	3.259830
307.452791	3619.552111	6.573363	-0.058957	3.263360
307.678112	3627.649264	6.578368	-0.059005	3.266929
308.349546	3635.624479	6.583373	-0.059135	3.270458
309.074096	3643.603740	6.588378	-0.059275	3.273987
309.276783	3651.700654	6.593382	-0.059318	3.277542
309.447393	3659.748034	6.598387	-0.059355	3.281071
310.208256	3667.719298	6.603392	-0.059502	3.284587
309.912355	3675.855583	6.608397	-0.059452	3.288128
310.075996	3683.910551	6.613402	-0.059488	3.291648
310.694071	3691.906287	6.618406	-0.059608	3.295157
310.569143	3699.966948	6.623411	-0.059590	3.298661
311.419599	3707.902349	6.628416	-0.059754	3.302145
311.232006	3716.022537	6.633421	-0.059724	3.305665
311.625436	3724.023922	6.638426	-0.059803	3.309152
312.066124	3732.049143	6.643430	-0.059890	3.312648
312.313110	3740.086783	6.648435	-0.059941	3.316138
312.509315	3748.141909	6.653440	-0.059983	3.319629
313.398377	3756.012696	6.658445	-0.060154	3.323064
313.871700	3764.062387	6.663450	-0.060247	3.326557
314.376473	3772.116522	6.668454	-0.060346	3.330049
314.638620	3780.171220	6.673459	-0.060400	3.333528
314.869794	3788.272792	6.678464	-0.060449	3.337022
315.184327	3796.300732	6.683469	-0.060512	3.340485
315.242553	3804.338719	6.688474	-0.060528	3.343938
315.250885	3812.425137	6.693478	-0.060535	3.347407
316.117347	3820.360588	6.698483	-0.060702	3.350839
317.049764	3828.292239	6.703488	-0.060881	3.354269
317.311300	3836.349691	6.708493	-0.060935	3.357724
317.964925	3844.368134	6.713498	-0.061062	3.361173
318.483979	3852.376126	6.718502	-0.061163	3.364609
318.229213	3860.526594	6.723507	-0.061121	3.368074
318.902024	3868.542439	6.728512	-0.061252	3.371512
319.212352	3876.529171	6.733517	-0.061315	3.374920
319.440720	3884.601787	6.738522	-0.061363	3.378359
319.781144	3892.657627	6.743526	-0.061431	3.381791
319.696384	3900.694322	6.748531	-0.061421	3.385196
319.834135	3908.750940	6.753536	-0.061452	3.388614
320.730414	3916.707982	6.758541	-0.061624	3.392013
321.107340	3924.739254	6.763546	-0.061699	3.395422
321.119459	3932.784002	6.768550	-0.061707	3.398820
321.580638	3940.763076	6.773555	-0.061798	3.402203
322.099969	3948.766874	6.778560	-0.061900	3.405595
322.577957	3956.763860	6.783565	-0.061994	3.408980
322.641737	3964.884220	6.788570	-0.062011	3.412398
322.325326	3973.012097	6.793574	-0.061957	3.415802
322.497362	3980.943916	6.798579	-0.061995	3.419138
323.113788	3988.954280	6.803584	-0.062115	3.422519
323.354982	3996.984888	6.808589	-0.062165	3.425892
323.828034	4004.932527	6.813594	-0.062258	3.429235
323.869292	4013.057841	6.818598	-0.062271	3.432634
324.114490	4021.082310	6.823603	-0.062322	3.435994
324.837054	4029.045235	6.828608	-0.062462	3.439342
324.981007	4037.066379	6.833613	-0.062494	3.442691
325.377503	4045.105315	6.838618	-0.062573	3.446053
325.895062	4053.143830	6.843622	-0.062675	3.449416
325.670907	4061.238586	6.848627	-0.062638	3.452773
326.577581	4069.204836	6.853632	-0.062812	3.456112
326.667684	4077.229408	6.858637	-0.062834	3.459444
327.089353	4085.239250	6.863642	-0.062918	3.462778
327.329995	4093.323041	6.868646	-0.062968	3.466133
327.491383	4101.355523	6.873651	-0.063003	3.469461
327.880786	4109.369781	6.878656	-0.063081	3.472786
328.155302	4117.393622	6.883661	-0.063137	3.476108
328.545160	4125.390233	6.888666	-0.063215	3.479419
328.895616	4133.424348	6.893670	-0.063286	3.482741
329.003955	4141.448539	6.898675	-0.063311	3.486048
329.421678	4149.500471	6.903680	-0.063394	3.489373
329.666119	4157.539141	6.908685	-0.063445	3.492684
329.536740	4165.636620	6.913690	-0.063426	3.496004
330.203274	4173.552115	6.918694	-0.063555	3.499271
330.663208	4181.580123	6.923699	-0.063646	3.502575
330.765386	4189.657933	6.928704	-0.063671	3.505885
331.230537	4197.632333	6.933709	-0.063762	3.509161
332.251630	4205.602815	6.938714	-0.063958	3.512450
332.117578	4213.762899	6.943718	-0.063938	3.515776
331.599999	4221.813582	6.948723	-0.063847	3.519042
332.334799	4229.776095	6.953728	-0.063989	3.522310
332.637398	4237.763103	6.958733	-0.064051	3.525570
333.261086	4245.741941	6.963738	-0.064172	3.528834
333.587995	4253.826794	6.968742	-0.064238	3.532129
334.258600	4261.806612	6.973747	-0.064368	3.535388
334.192562	4269.898626	6.978752	-0.064361	3.538667
334.595021	4277.925110	6.983757	-0.064441	3.541931
335.024701	4285.899223	6.988762	-0.064527	3.545172
335.716260	4293.895575	6.993766	-0.064661	3.548427
335.889104	4302.015698	6.998771	-0.064698	3.551712
335.505355	4310.160999	7.003776	-0.064632	3.554988
336.270619	4318.057603	7.008781	-0.064780	3.558195
336.682886	4325.991503	7.013786	-0.064861	3.561404
337.043991	4333.976968	7.018790	-0.064934	3.564629
337.429936	4342.036321	7.023795	-0.065011	3.567882
337.884790	4350.153240	7.028800	-0.065101	3.571156
337.954882	4358.176684	7.033805	-0.065119	3.574379
338.268053	4366.219629	7.038810	-0.065183	3.577614
338.792040	4374.210641	7.043814	-0.065286	3.580831
338.860982	4382.173450	7.048819	-0.065304	3.584020
339.672149	4390.225844	7.053824	-0.065460	3.587265
339.908408	4398.259607	7.058829	-0.065509	3.590482
340.399124	4406.257678	7.063834	-0.065606	3.593689
340.763574	4414.342890	7.068838	-0.065679	3.596924
340.782404	4422.371539	7.073843	-0.065688	3.600124
341.674305	4430.329381	7.078848	-0.065859	3.603318
341.680914	4438.361616	7.083853	-0.065866	3.606513
342.127573	4446.394915	7.088858	-0.065954	3.609719
342.547681	4454.454011	7.093862	-0.066037	3.612930
342.951593	4462.469683	7.098867	-0.066118	3.616122
343.398828	4470.472952	7.103872	-0.066206	3.619306
343.548790	4478.536420	7.108877	-0.066240	3.622504
344.035733	4486.534750	7.113882	-0.066335	3.625682
343.914186	4494.654982	7.118886	-0.066318	3.628888
344.302843	4502.613073	7.123891	-0.066396	3.632042
344.018891	4510.733783	7.128896	-0.066348	3.635238
344.548775	4518.634217	7.133901	-0.066452	3.638368
344.812106	4526.665233	7.138906	-0.066506	3.641539
345.280641	4534.683335	7.143910	-0.066599	3.644707
345.393352	4542.670926	7.148915	-0.066625	3.647851
345.652245	4550.787180	7.153920	-0.066678	3.651047
346.105014	4558.773761	7.158925	-0.066768	3.654194
346.624261	4566.764392	7.163930	-0.066870	3.657342
346.747165	4574.826401	7.168934	-0.066898	3.660504
347.235132	4582.763998	7.173939	-0.066994	3.663625
347.949377	4590.820690	7.178944	-0.067132	3.666796
347.831516	4598.928524	7.183949	-0.067116	3.669961
347.641453	4606.983489	7.188954	-0.067086	3.673101
348.249942	4614.978463	7.193958	-0.067204	3.676237
348.182214	4622.991558	7.198963	-0.067197	3.679358
348.551233	4630.984040	7.203968	-0.067271	3.682481
349.184629	4638.973518	7.208973	-0.067394	3.685607
349.325733	4646.993023	7.213978	-0.067425	3.688728
349.529811	4655.066589	7.218982	-0.067469	3.691870
349.922940	4663.064371	7.223987	-0.067547	3.694984
350.344358	4671.101008	7.228992	-0.067631	3.698112
350.179046	4679.202528	7.233997	-0.067605	3.701247
350.479907	4687.147372	7.239002	-0.067666	3.704331
351.398786	4695.136905	7.244006	-0.067843	3.707445
351.234837	4703.245956	7.249011	-0.067818	3.710575
351.774304	4711.312744	7.254016	-0.067923	3.713703
352.109926	4719.288341	7.259021	-0.067991	3.716789
352.501086	4727.250050	7.264026	-0.068069	3.719868
352.908397	4735.267748	7.269030	-0.068150	3.722967
353.004752	4743.317549	7.274035	-0.068173	3.726067
353.625916	4751.283794	7.279040	-0.068294	3.729146
353.490420	4759.422408	7.284045	-0.068274	3.732270
353.290117	4767.461346	7.289050	-0.068242	3.735351
353.858629	4775.396022	7.294054	-0.068353	3.738409
354.166979	4783.438989	7.299059	-0.068416	3.741499
354.053629	4791.470197	7.304064	-0.068400	3.744572
353.985619	4799.549132	7.309069	-0.068393	3.747661
354.609226	4807.506350	7.314074	-0.068514	3.750718
355.226002	4815.476502	7.319078	-0.068634	3.753778
355.794303	4823.471247	7.324083	-0.068745	3.756843
356.399977	4831.469594	7.329088	-0.068863	3.759908
356.232989	4839.571070	7.334093	-0.068837	3.762991
356.301906	4847.608492	7.339098	-0.068855	3.766053
356.915662	4855.633080	7.344102	-0.068975	3.769120
357.186608	4863.651418	7.349107	-0.069031	3.772174
357.659893	4871.652251	7.354112	-0.069124	3.775224
358.004934	4879.646343	7.359117	-0.069193	3.778266
358.226001	4887.723909	7.364122	-0.069240	3.781334
358.157413	4895.758435	7.369126	-0.069232	3.784376
358.531967	4903.786141	7.374131	-0.069307	3.787424
358.781153	4911.838915	7.379136	-0.069359	3.790476
359.113885	4919.846907	7.384141	-0.069426	3.793510
359.352883	4927.861391	7.389146	-0.069476	3.796542
359.713447	4935.822030	7.394150	-0.069548	3.799554
359.442690	4943.892849	7.399155	-0.069503	3.802591
360.029027	4951.876785	7.404160	-0.069617	3.805612
360.617502	4959.834012	7.409165	-0.069732	3.808621
360.917106	4967.905643	7.414170	-0.069793	3.811664
361.147774	4975.964718	7.419174	-0.069841	3.814698
361.650120	4983.940928	7.424179	-0.069940	3.817704
362.222862	4991.984396	7.429184	-0.070052	3.820735
361.524087	5000.127310	7.434189	-0.069927	3.823772
361.977684	5008.124171	7.439194	-0.070017	3.826778
362.265972	5016.128072	7.444198	-0.070076	3.829781
362.405290	5024.133762	7.449203	-0.070107	3.832778
362.805321	5032.158127	7.454208	-0.070187	3.835786
362.965103	5040.162823	7.459213	-0.070222	3.838779
363.261025	5048.201092	7.464218	-0.070282	3.841784
363.267222	5056.201407	7.469222	-0.070289	3.844768
363.249388	5064.226098	7.474227	-0.070290	3.847757
363.544221	5072.306176	7.479232	-0.070351	3.850771
363.774959	5080.255335	7.484237	-0.070399	3.853733
364.563224	5088.241914	7.489242	-0.070551	3.856718
364.850238	5096.280363	7.494246	-0.070609	3.859710
365.425830	5104.235602	7.499251	-0.070722	3.862674
365.227202	5112.364758	7.504256	-0.070690	3.865684
365.867863	5120.322271	7.509261	-0.070815	3.868646
366.441872	5128.408008	7.514266	-0.070927	3.871652
366.944218	5136.489096	7.519270	-0.071026	3.874652
366.776744	5144.497388	7.524275	-0.071000	3.877609
367.056447	5152.453929	7.529280	-0.071057	3.880553
367.073829	5160.454845	7.534285	-0.071065	3.883507
366.975113	5168.526697	7.539290	-0.071052	3.886482
367.494019	5176.509756	7.544294	-0.071154	3.889434
367.934349	5184.487298	7.549299	-0.071241	3.892381
368.304775	5192.489323	7.554304	-0.071316	3.895332
368.267143	5200.541845	7.559309	-0.071314	3.898292
369.164852	5208.531983	7.564314	-0.071486	3.901246
369.372933	5216.517283	7.569318	-0.071530	3.904181
369.181769	5224.594855	7.574323	-0.071500	3.907141
369.588018	5232.654149	7.579328	-0.071581	3.910103
369.826766	5240.650228	7.584333	-0.071630	3.913036
369.755988	5248.771273	7.589338	-0.071623	3.916007
370.324117	5256.703217	7.594342	-0.071734	3.918919
370.821324	5264.673256	7.599347	-0.071831	3.921841
371.482616	5272.671623	7.604352	-0.071960	3.924775
371.001226	5280.861942	7.609357	-0.071875	3.927754
371.909815	5288.775027	7.614362	-0.072050	3.930657
371.874650	5296.871147	7.619366	-0.072048	3.933606
372.029977	5304.861383	7.624371	-0.072083	3.936518
372.671356	5312.823086	7.629376	-0.072207	3.939426
373.230435	5320.832988	7.634381	-0.072317	3.942348
372.876199	5328.907025	7.639386	-0.072256	3.945275
373.199982	5336.942000	7.644390	-0.072321	3.948197
373.293281	5345.004258	7.649395	-0.072344	3.951123
373.672581	5352.993434	7.654400	-0.072420	3.954025
374.295407	5360.956536	7.659405	-0.072541	3.956921
374.600786	5368.987427	7.664410	-0.072603	3.959833
374.672193	5377.039528	7.669414	-0.072622	3.962746
375.129815	5385.031674	7.674419	-0.072712	3.965642
375.701403	5392.970582	7.679424	-0.072824	3.968519
376.103030	5401.055471	7.684429	-0.072904	3.971443
375.647562	5409.152328	7.689434	-0.072824	3.974355
375.825059	5417.185745	7.694438	-0.072863	3.977252
376.298935	5425.107394	7.699443	-0.072956	3.980113
376.059330	5433.207698	7.704448	-0.072917	3.983023
376.169596	5441.197838	7.709453	-0.072942	3.985897
376.303019	5449.233541	7.714458	-0.072973	3.988786
376.795923	5457.272641	7.719462	-0.073070	3.991681
377.228113	5465.188364	7.724467	-0.073155	3.994528
377.576027	5473.252475	7.729472	-0.073225	3.997424
377.446011	5481.314771	7.734477	-0.073206	4.000310
377.285538	5489.336292	7.739482	-0.073182	4.003178
378.002522	5497.329160	7.744486	-0.073320	4.006049
378.089305	5505.321809	7.749491	-0.073342	4.008907
378.903038	5513.329971	7.754496	-0.073499	4.011781
379.292960	5521.300936	7.759501	-0.073576	4.014633
379.384618	5529.405397	7.764506	-0.073599	4.017525
379.016429	5537.536076	7.769510	-0.073536	4.020416
378.903464	5545.509902	7.774515	-0.073520	4.023254
379.436563	5553.494874	7.779520	-0.073624	4.026104
379.706368	5561.524951	7.784525	-0.073680	4.028964
379.561974	5569.600728	7.789530	-0.073658	4.031832
379.916422	5577.609551	7.794534	-0.073729	4.034682
380.492925	5585.528842	7.799539	-0.073842	4.037501
380.591279	5593.621517	7.804544	-0.073865	4.040373
380.823914	5601.567711	7.809549	-0.073914	4.043192
380.604420	5609.648098	7.814554	-0.073878	4.046050
381.606993	5617.558335	7.819558	-0.074070	4.048865
381.629722	5625.655376	7.824563	-0.074080	4.051728
381.785572	5633.683394	7.829568	-0.074114	4.054567
382.820576	5641.586811	7.834573	-0.074312	4.057374
383.027119	5649.622368	7.839578	-0.074356	4.060213
382.678280	5657.748744	7.844582	-0.074296	4.063073
383.029332	5665.709685	7.849587	-0.074366	4.065883
383.426309	5673.753263	7.854592	-0.074446	4.068721
383.221708	5681.882406	7.859597	-0.074413	4.071579
383.238431	5689.831928	7.864602	-0.074421	4.074374
383.572172	5697.865978	7.869606	-0.074489	4.077202
384.237379	5705.793985	7.874611	-0.074618	4.079995
384.830028	5713.801062	7.879616	-0.074733	4.082814
385.353663	5721.832834	7.884621	-0.074836	4.085638
386.045187	5729.809065	7.889626	-0.074970	4.088442
386.642636	5737.889497	7.894630	-0.075086	4.091280
386.567951	5745.891806	7.899635	-0.075078	4.094079
386.880707	5753.963238	7.904640	-0.075141	4.096906
387.101794	5761.975286	7.909645	-0.075188	4.099708
387.107088	5770.024005	7.914650	-0.075194	4.102519
387.740688	5778.000154	7.919654	-0.075317	4.105311
387.607304	5786.059303	7.924659	-0.075297	4.108119
388.090706	5794.081406	7.929664	-0.075393	4.110921
388.489522	5802.078465	7.934669	-0.075472	4.113711
388.486357	5810.133791	7.939674	-0.075477	4.116514
388.909242	5818.088068	7.944678	-0.075561	4.119286
388.864348	5826.112001	7.949683	-0.075558	4.122074
389.236596	5834.132329	7.954688	-0.075632	4.124864
388.781469	5842.244258	7.959693	-0.075553	4.127673
389.147512	5850.188530	7.964698	-0.075626	4.130432
389.503326	5858.226081	7.969702	-0.075698	4.133223
389.952846	5866.220558	7.974707	-0.075787	4.135997
390.178037	5874.242638	7.979712	-0.075834	4.138776
390.603914	5882.240067	7.984717	-0.075918	4.141548
390.864123	5890.175153	7.989722	-0.075972	4.144293
391.303004	5898.289799	7.994726	-0.076059	4.147102
391.735864	5906.268295	7.999731	-0.076145	4.149861
391.819823	5914.319501	8.004736	-0.076166	4.152639
391.781232	5922.368863	8.009741	-0.076164	4.155413
391.696157	5930.420760	8.014746	-0.076153	4.158185
392.205083	5938.448250	8.019750	-0.076253	4.160955
392.370268	5946.383874	8.024755	-0.076289	4.163686
392.230509	5954.482928	8.029760	-0.076268	4.166469
392.732874	5962.408924	8.034765	-0.076367	4.169198
393.006925	5970.445788	8.039770	-0.076423	4.171960
393.392446	5978.491441	8.044774	-0.076500	4.174725
393.550882	5986.484081	8.049779	-0.076535	4.177467
394.246356	5994.469645	8.054784	-0.076670	4.180211
394.617361	6002.508522	8.059789	-0.076744	4.182968
394.397735	6010.611624	8.064794	-0.076709	4.185738
394.804828	6018.639091	8.069798	-0.076790	4.188487
395.094630	6026.622094	8.074803	-0.076849	4.191218
395.292086	6034.731552	8.079808	-0.076891	4.193990
395.762071	6042.694482	8.084813	-0.076984	4.196713
396.339508	6050.556602	8.089818	-0.077096	4.199400
396.607453	6058.661610	8.094822	-0.077151	4.202165
396.483508	6066.658542	8.099827	-0.077134	4.204887
396.876228	6074.705951	8.104832	-0.077212	4.207631
397.270959	6082.710051	8.109837	-0.077291	4.210358
397.446105	6090.748725	8.114842	-0.077329	4.213092
398.160850	6098.737508	8.119846	-0.077467	4.215813
398.548522	6106.699974	8.124851	-0.077544	4.218520
398.516212	6114.863460	8.129856	-0.077544	4.221289
398.619924	6122.794897	8.134861	-0.077568	4.223979
398.947636	6130.845111	8.139866	-0.077634	4.226710
398.956626	6138.885790	8.144870	-0.077641	4.229432
398.949072	6146.899873	8.149875	-0.077645	4.232144
399.296609	6154.899759	8.154880	-0.077715	4.234852
399.928372	6162.884130	8.159885	-0.077838	4.237557
400.216972	6170.903813	8.164890	-0.077897	4.240268
400.442120	6178.923285	8.169894	-0.077944	4.242977
400.766541	6186.947753	8.174899	-0.078010	4.245686
400.647197	6194.992689	8.179904	-0.077993	4.248397
401.259928	6203.010646	8.184909	-0.078112	4.251103
401.181505	6211.040572	8.189914	-0.078103	4.253806
401.849778	6219.058201	8.194918	-0.078232	4.256509
402.153164	6226.992496	8.199923	-0.078294	4.259179
401.937226	6235.127352	8.204928	-0.078259	4.261910
402.404679	6243.050393	8.209933	-0.078351	4.264575
402.683747	6251.068696	8.214938	-0.078409	4.267268
402.915508	6259.159662	8.219942	-0.078457	4.269983
403.106019	6267.149872	8.224947	-0.078498	4.272662
403.269421	6275.168327	8.229952	-0.078533	4.275349
403.916872	6283.131724	8.234957	-0.078659	4.278020
404.022924	6291.218095	8.239962	-0.078684	4.280726
404.330806	6299.222789	8.244966	-0.078747	4.283404
404.507331	6307.211908	8.249971	-0.078785	4.286075
404.640810	6315.254032	8.254976	-0.078815	4.288760
405.215473	6323.287500	8.259981	-0.078927	4.291446
405.378749	6331.214538	8.264986	-0.078963	4.294090
405.991406	6339.246139	8.269990	-0.079082	4.296771
406.016517	6347.246918	8.274995	-0.079092	4.299436
405.795642	6355.414900	8.280000	-0.079056	4.302152
405.957263	6363.320726	8.285005	-0.079091	4.304783
406.692619	6371.311576	8.290010	-0.079234	4.307445
407.062806	6379.366849	8.295014	-0.079308	4.310123
407.282909	6387.383118	8.300019	-0.079354	4.312786
407.230845	6395.412235	8.305024	-0.079349	4.315449
407.575755	6403.436377	8.310029	-0.079419	4.318112
407.830387	6411.415073	8.315034	-0.079472	4.320758
408.236619	6419.389382	8.320038	-0.079552	4.323402
408.223933	6427.440311	8.325043	-0.079555	4.326066
408.353711	6435.514477	8.330048	-0.079585	4.328737
408.379279	6443.571624	8.335053	-0.079595	4.331400
408.913280	6451.508177	8.340058	-0.079699	4.334025
409.580817	6459.571498	8.345062	-0.079829	4.336692
409.706719	6467.495596	8.350067	-0.079858	4.339307
409.901216	6475.574502	8.355072	-0.079899	4.341972
410.162770	6483.559284	8.360077	-0.079953	4.344605
410.424387	6491.578423	8.365082	-0.080007	4.347247
410.580128	6499.637218	8.370086	-0.080041	4.349900
411.036829	6507.713242	8.375091	-0.080132	4.352560
411.606353	6515.665512	8.380096	-0.080243	4.355178
411.626725	6523.710025	8.385101	-0.080252	4.357820
411.659458	6531.636441	8.390106	-0.080263	4.360422
412.284532	6539.630935	8.395110	-0.080385	4.363049
412.521744	6547.646453	8.400115	-0.080434	4.365679
412.628725	6555.669677	8.405120	-0.080459	4.368309
413.137674	6563.757981	8.410125	-0.080559	4.370961
413.354037	6571.704837	8.415130	-0.080605	4.373563
413.443956	6579.827188	8.420134	-0.080627	4.376220
413.676975	6587.775789	8.425139	-0.080675	4.378820
413.938270	6595.827109	8.430144	-0.080729	4.381452
413.997590	6603.799437	8.435149	-0.080746	4.384055
414.185330	6611.855336	8.440154	-0.080786	4.386685
414.688325	6619.915688	8.445158	-0.080885	4.389316
414.788426	6627.958281	8.450163	-0.080909	4.391938
414.917422	6635.918869	8.455168	-0.080938	4.394531
415.281037	6643.958409	8.460173	-0.081011	4.397150
415.566837	6651.917005	8.465178	-0.081069	4.399741
415.848881	6659.975584	8.470182	-0.081127	4.402362
416.235515	6667.942954	8.475187	-0.081204	4.404953
416.358363	6676.013304	8.480192	-0.081232	4.407574
416.473887	6684.103084	8.485197	-0.081259	4.410200
416.567847	6692.133612	8.490202	-0.081282	4.412805
417.272777	6700.127255	8.495206	-0.081418	4.415400
417.458724	6708.096437	8.500211	-0.081458	4.417983
417.395784	6716.208768	8.505216	-0.081452	4.420609
417.551702	6724.194742	8.510221	-0.081486	4.423194
417.578414	6732.232074	8.515226	-0.081496	4.425793
418.055632	6740.209579	8.520230	-0.081590	4.428373
418.495245	6748.197395	8.525235	-0.081677	4.430955
418.564801	6756.254164	8.530240	-0.081696	4.433556
419.175209	6764.284683	8.535245	-0.081815	4.436150
418.856236	6772.291420	8.540250	-0.081760	4.438730
419.183712	6780.408795	8.545254	-0.081827	4.441347
419.146544	6788.283668	8.550259	-0.081825	4.443883
419.958626	6796.277067	8.555264	-0.081981	4.446459
420.373779	6804.322249	8.560269	-0.082064	4.449049
420.657294	6812.349980	8.565274	-0.082122	4.451631
421.325500	6820.341802	8.570279	-0.082252	4.454202
421.356482	6828.453846	8.575283	-0.082263	4.456806
421.345792	6836.413594	8.580288	-0.082266	4.459360
421.285862	6844.526624	8.585293	-0.082260	4.461962
421.373000	6852.410416	8.590298	-0.082281	4.464489
421.899360	6860.494445	8.595303	-0.082385	4.467081
422.076152	6868.489631	8.600307	-0.082423	4.469641
422.714656	6876.456920	8.605312	-0.082547	4.472193
422.890726	6884.493744	8.610317	-0.082585	4.474764
423.446575	6892.505882	8.615322	-0.082694	4.477327
423.876655	6900.507835	8.620327	-0.082779	4.479884
423.898719	6908.525572	8.625331	-0.082788	4.482444
424.461806	6916.543126	8.630336	-0.082898	4.485004
424.654516	6924.578849	8.635341	-0.082939	4.487567
424.682368	6932.582038	8.640346	-0.082950	4.490117
424.924831	6940.647065	8.645351	-0.083000	4.492686
425.042863	6948.656453	8.650355	-0.083028	4.495236
425.119084	6956.710191	8.655360	-0.083047	4.497798
425.267070	6964.724530	8.660365	-0.083080	4.500347
425.568314	6972.612045	8.665370	-0.083141	4.502854
426.080379	6980.685678	8.670375	-0.083242	4.505420
426.280009	6988.720238	8.675379	-0.083284	4.507971
426.641851	6996.712444	8.680384	-0.083357	4.510507
427.235075	7004.704945	8.685389	-0.083472	4.513043
427.067610	7012.740429	8.690394	-0.083446	4.515588
427.592508	7020.718295	8.695399	-0.083549	4.518116
427.817690	7028.758031	8.700403	-0.083597	4.520661
427.506772	7036.761095	8.705408	-0.083544	4.523191
427.748726	7044.859193	8.710413	-0.083594	4.525752
428.159592	7052.766702	8.715418	-0.083676	4.528251
428.648364	7060.826404	8.720423	-0.083772	4.530798
428.713051	7068.822310	8.725427	-0.083789	4.533321
428.888074	7076.866317	8.730432	-0.083827	4.535859
429.003273	7084.906489	8.735437	-0.083854	4.538394
428.903779	7092.968820	8.740442	-0.083841	4.540933
429.529417	7100.892001	8.745447	-0.083962	4.543430
429.691380	7108.909729	8.750451	-0.083998	4.545953
429.614159	7116.955637	8.755456	-0.083989	4.548484
429.885715	7125.009393	8.760461	-0.084044	4.551016
430.353833	7132.937115	8.765466	-0.084137	4.553507
430.731512	7141.030130	8.770471	-0.084212	4.556049
430.967751	7148.979510	8.775475	-0.084262	4.558545
431.078884	7157.013826	8.780480	-0.084288	4.561065
431.357126	7165.013710	8.785485	-0.084345	4.563573
431.528247	7173.064631	8.790490	-0.084382	4.566095
431.813510	7181.064538	8.795495	-0.084440	4.568601
432.095976	7189.114878	8.800499	-0.084498	4.571121
432.420782	7197.074685	8.805504	-0.084564	4.573611
432.698780	7205.174089	8.810509	-0.084621	4.576143
432.430580	7213.143005	8.815514	-0.084576	4.578632
432.385338	7221.244055	8.820519	-0.084573	4.581162
432.725780	7229.122557	8.825523	-0.084641	4.583621
433.430867	7237.160932	8.830528	-0.084778	4.586129
433.474529	7245.190901	8.835533	-0.084791	4.588632
433.590993	7253.198910	8.840538	-0.084818	4.591127
434.005377	7261.239207	8.845543	-0.084901	4.593631
434.201595	7269.260819	8.850547	-0.084942	4.596128
434.606291	7277.179692	8.855552	-0.085023	4.598592
434.975453	7285.265837	8.860557	-0.085097	4.601106
435.273305	7293.186927	8.865562	-0.085158	4.603567
435.243563	7301.320550	8.870567	-0.085157	4.606093
435.096296	7309.304017	8.875571	-0.085135	4.608571
435.363613	7317.401360	8.880576	-0.085190	4.611083
435.521988	7325.366511	8.885581	-0.085225	4.613552
435.240143	7333.416625	8.890586	-0.085178	4.616046
435.613235	7341.398024	8.895591	-0.085252	4.618518
435.825995	7349.453774	8.900595	-0.085297	4.621012
436.544487	7357.300104	8.905600	-0.085436	4.623439
437.056023	7365.412755	8.910605	-0.085537	4.625948
436.883227	7373.399538	8.915610	-0.085510	4.628416
437.125944	7381.504319	8.920615	-0.085560	4.630919
437.150985	7389.465071	8.925619	-0.085570	4.633376
437.845912	7397.472095	8.930624	-0.085705	4.635847
438.106675	7405.480861	8.935629	-0.085758	4.638316
438.181160	7413.536625	8.940634	-0.085778	4.640799
438.132247	7421.503481	8.945639	-0.085774	4.643253
438.530512	7429.538474	8.950643	-0.085853	4.645726
438.516959	7437.567659	8.955648	-0.085856	4.648197
438.643284	7445.632661	8.960653	-0.085885	4.650677
438.634176	7453.544452	8.965658	-0.085888	4.653109
439.179710	7461.614354	8.970663	-0.085995	4.655588
439.239033	7469.616059	8.975667	-0.086011	4.658044
439.382862	7477.620087	8.980672	-0.086043	4.660500
439.815197	7485.666487	8.985677	-0.086129	4.662968
440.156540	7493.646884	8.990682	-0.086198	4.665414
440.295470	7501.703612	8.995687	-0.086229	4.667882
440.058286	7509.778187	9.000691	-0.086190	4.670355
440.707445	7517.747693	9.005696	-0.086316	4.672794
441.062620	7525.788297	9.010701	-0.086387	4.675253
440.785332	7533.748896	9.015706	-0.086341	4.677687
441.909845	7541.715417	9.020711	-0.086556	4.680120
441.972409	7549.703801	9.025715	-0.086572	4.682560
442.225290	7557.704152	9.030720	-0.086625	4.685001
442.595627	7565.828947	9.035725	-0.086699	4.687479
442.874185	7573.798092	9.040730	-0.086756	4.689909
442.999375	7581.873378	9.045735	-0.086785	4.692370
443.087318	7589.856437	9.050739	-0.086806	4.694801
443.575262	7597.838163	9.055744	-0.086902	4.697230
443.735983	7605.896686	9.060749	-0.086938	4.699682
443.786585	7613.904561	9.065754	-0.086952	4.702117
444.331519	7621.861429	9.070759	-0.087059	4.704535
444.603915	7629.944616	9.075763	-0.087115	4.706990
444.684937	7637.929330	9.080768	-0.087135	4.709414
445.058619	7645.981503	9.085773	-0.087210	4.711857
445.297855	7653.928128	9.090778	-0.087260	4.714267
445.243275	7662.047202	9.095783	-0.087255	4.716729
445.291033	7670.014452	9.100787	-0.087269	4.719143
445.919972	7678.027523	9.105792	-0.087391	4.721568
446.338395	7685.976571	9.110797	-0.087474	4.723973
446.259880	7694.062860	9.115802	-0.087465	4.726420
446.522875	7702.092608	9.120807	-0.087519	4.728847
446.795643	7710.144226	9.125811	-0.087575	4.731280
446.803748	7718.108274	9.130816	-0.087582	4.733685
446.883065	7726.220685	9.135821	-0.087602	4.736134
447.183561	7734.105095	9.140826	-0.087663	4.738512
447.287983	7742.230240	9.145831	-0.087688	4.740963
447.171345	7750.205599	9.150835	-0.087672	4.743367
447.709803	7758.216176	9.155840	-0.087777	4.745779
447.841015	7766.277452	9.160845	-0.087807	4.748206
447.764656	7774.271632	9.165850	-0.087798	4.750612
448.358566	7782.247625	9.170855	-0.087914	4.753010
448.465873	7790.297314	9.175859	-0.087939	4.755430
448.609646	7798.272504	9.180864	-0.087971	4.757826
448.781743	7806.359132	9.185869	-0.088008	4.760254
449.180549	7814.329355	9.190874	-0.088088	4.762645
449.283944	7822.298813	9.195879	-0.088112	4.765036
449.437327	7830.372781	9.200883	-0.088146	4.767457
449.707724	7838.338531	9.205888	-0.088201	4.769844
450.216444	7846.447378	9.210893	-0.088301	4.772272
450.182439	7854.361952	9.215898	-0.088300	4.774641
450.545669	7862.466237	9.220903	-0.088373	4.777066
450.696212	7870.408577	9.225907	-0.088406	4.779441
450.772757	7878.504530	9.230912	-0.088426	4.781861
451.200869	7886.454941	9.235917	-0.088511	4.784235
451.371086	7894.524683	9.240922	-0.088548	4.786645
451.523540	7902.519899	9.245927	-0.088581	4.789031
451.801008	7910.576117	9.250931	-0.088638	4.791434
452.014397	7918.467129	9.255936	-0.088683	4.793786
452.392590	7926.577847	9.260941	-0.088759	4.796202
452.283272	7934.512761	9.265946	-0.088744	4.798567
452.747648	7942.581478	9.270951	-0.088836	4.800967
452.538317	7950.572361	9.275955	-0.088802	4.803346
452.436463	7958.665110	9.280960	-0.088788	4.805754
452.980550	7966.624397	9.285965	-0.088895	4.808118
453.245492	7974.636629	9.290970	-0.088949	4.810498
453.355489	7982.681329	9.295975	-0.088975	4.812887
453.353193	7990.128951	9.300979	-0.088979	4.815098
453.646877	7994.854519	9.305984	-0.089037	4.816499

454.146361	7997.413230	9.310989	-0.089132	4.817256
454.194652	7998.626277	9.315994	-0.089142	4.817616
454.344885	7999.471409	9.320999	-0.089170	4.817866
454.633736	7999.814359	9.326003	-0.089224	4.817967
454.598036	8000.518021	9.331008	-0.089218	4.818176
454.373009	8000.448560	9.336013	-0.089176	4.818156
454.712612	8000.482787	9.341018	-0.089239	4.818165
454.804379	8000.441970	9.346023	-0.089256	4.818152
455.069469	8000.522522	9.351027	-0.089306	4.818175
455.158395	8000.395353	9.356032	-0.089322	4.818137
455.518113	8000.490915	9.361037	-0.089389	4.818164
455.407487	8000.475682	9.366042	-0.089369	4.818160
455.812337	8000.386620	9.371047	-0.089444	4.818132
456.130902	8000.458451	9.376051	-0.089503	4.818152
455.859386	8000.467279	9.381056	-0.089453	4.818155
456.076151	8000.492422	9.386061	-0.089493	4.818162
456.206696	8000.420569	9.391066	-0.089518	4.818140
456.226655	8000.476638	9.396071	-0.089521	4.818157
456.473278	8000.459043	9.401075	-0.089567	4.818150
456.294886	8000.343914	9.406080	-0.089534	4.818117
456.356974	8000.459520	9.411085	-0.089546	4.818151
456.407574	8000.413915	9.416090	-0.089555	4.818137
456.602087	8000.449273	9.421095	-0.089591	4.818147
456.736187	8000.439574	9.426099	-0.089616	4.818143
456.710968	8000.439222	9.431104	-0.089612	4.818143
456.809890	8000.450083	9.436109	-0.089630	4.818146
456.758600	8000.428313	9.441114	-0.089620	4.818140
456.762795	8000.467320	9.446119	-0.089621	4.818152
456.837214	8000.443101	9.451123	-0.089635	4.818144
456.899020	8000.474494	9.456128	-0.089647	4.818153
457.207502	8000.477767	9.461133	-0.089704	4.818153
456.680902	8000.401966	9.466138	-0.089606	4.818133
457.005973	8000.501259	9.471143	-0.089667	4.818161
457.030223	8000.454232	9.476147	-0.089671	4.818147
456.722321	8000.409917	9.481152	-0.089614	4.818135
456.755475	8000.453541	9.486157	-0.089620	4.818147
456.726913	8000.420510	9.491162	-0.089615	4.818138
457.158365	8000.440242	9.496167	-0.089695	4.818142
457.225372	8000.527499	9.501171	-0.089708	4.818167
457.215728	8000.433680	9.506176	-0.089706	4.818140
457.248221	8000.486768	9.511181	-0.089712	4.818155
457.161012	8000.412915	9.516186	-0.089696	4.818134
456.820462	8000.324985	9.521191	-0.089632	4.818109
457.095631	8000.355158	9.526195	-0.089683	4.818117
457.240357	8000.438241	9.531200	-0.089710	4.818141
457.273716	8000.393446	9.536205	-0.089717	4.818128
457.355804	8000.528283	9.541210	-0.089732	4.818167
457.438386	8000.447336	9.546215	-0.089747	4.818143
457.322386	8000.440447	9.551219	-0.089726	4.818141
457.434980	8000.392552	9.556224	-0.089747	4.818127
457.723143	8000.497648	9.561229	-0.089800	4.818157
457.549629	8000.531006	9.566234	-0.089768	4.818167
457.549448	8000.353107	9.571239	-0.089768	4.818114
457.560169	8000.443786	9.576243	-0.089770	4.818141
457.447527	8000.435892	9.581248	-0.089749	4.818139
457.809788	8000.418866	9.586253	-0.089817	4.818133
457.397154	8000.521504	9.591258	-0.089740	4.818165
457.491001	8000.245976	9.596263	-0.089757	4.818083
457.663227	8000.421025	9.601267	-0.089789	4.818134
457.519992	8000.501124	9.606272	-0.089763	4.818158
457.917897	8000.449861	9.611277	-0.089837	4.818142
457.589235	8000.528413	9.616282	-0.089776	4.818166
457.734273	8000.432551	9.621287	-0.089803	4.818137
457.772769	8000.432039	9.626291	-0.089810	4.818137
457.776041	8000.420507	9.631296	-0.089810	4.818133
458.178408	8000.456678	9.636301	-0.089885	4.818142
458.047122	8000.401152	9.641306	-0.089861	4.818127
458.339645	8000.503153	9.646311	-0.089915	4.818156
457.720609	8000.339732	9.651315	-0.089800	4.818110
457.142815	8000.174793	9.656320	-0.089692	4.818063
457.787517	8000.285935	9.661325	-0.089813	4.818093
457.782817	8000.485873	9.666330	-0.089812	4.818153
457.643603	8000.330236	9.671335	-0.089786	4.818107
457.534860	8000.121344	9.676339	-0.089765	4.818046
457.921753	8000.357295	9.681344	-0.089838	4.818114
458.111851	8000.366278	9.686349	-0.089873	4.818116
458.098924	8000.447152	9.691354	-0.089871	4.818140
458.523458	8000.437318	9.696359	-0.089950	4.818135
458.446264	8000.481501	9.701363	-0.089935	4.818149
457.942223	8000.337587	9.706368	-0.089842	4.818108
457.931901	8000.377444	9.711373	-0.089840	4.818120
458.136275	8000.409785	9.716378	-0.089878	4.818129
457.999251	8000.137334	9.721383	-0.089852	4.818049
458.319088	8000.414456	9.726387	-0.089912	4.818129
458.035911	8000.282062	9.731392	-0.089859	4.818091
458.076189	8000.356314	9.736397	-0.089867	4.818113
457.902528	8000.371775	9.741402	-0.089834	4.818118
458.113838	8000.233683	9.746407	-0.089873	4.818077
458.709949	8000.439945	9.751411	-0.089985	4.818135
458.568721	8000.335855	9.756416	-0.089958	4.818105
458.351813	8000.311761	9.761421	-0.089918	4.818099
458.088177	8000.270170	9.766426	-0.089869	4.818088
458.345670	8000.365363	9.771431	-0.089917	4.818115
458.452949	8000.443713	9.776435	-0.089937	4.818137
458.593719	8000.459373	9.781440	-0.089963	4.818142
458.502284	8000.290718	9.786445	-0.089946	4.818092
458.250884	8000.360879	9.791450	-0.089899	4.818114
458.407147	8000.231490	9.796455	-0.089928	4.818075
458.307487	8000.077459	9.801459	-0.089910	4.818029
458.233128	8000.179577	9.806464	-0.089896	4.818060
458.503689	8000.313901	9.811469	-0.089946	4.818099
458.556512	8000.396751	9.816474	-0.089956	4.818123
458.750387	8000.269993	9.821479	-0.089992	4.818085
458.807212	8000.526591	9.826483	-0.090003	4.818161
458.745515	8000.364667	9.831488	-0.089991	4.818113
458.806832	8000.356054	9.836493	-0.090003	4.818110
458.268146	8000.185338	9.841498	-0.089902	4.818062
458.084844	8000.200664	9.846503	-0.089868	4.818067
458.222717	8000.205756	9.851507	-0.089894	4.818068
458.440021	8000.316175	9.856512	-0.089935	4.818100
458.294453	8000.254133	9.861517	-0.089907	4.818082
458.899794	8000.473158	9.866522	-0.090020	4.818144
458.862198	8000.251570	9.871527	-0.090013	4.818079
458.766442	8000.389180	9.876531	-0.089995	4.818120
458.818971	8000.361496	9.881536	-0.090005	4.818112
458.884089	8000.329778	9.886541	-0.090017	4.818102
458.501584	8000.192831	9.891546	-0.089946	4.818063
458.855438	8000.302008	9.896551	-0.090012	4.818094
459.059694	8000.368035	9.901555	-0.090050	4.818113
458.533944	8000.229078	9.906560	-0.089952	4.818073
458.417459	8000.241130	9.911565	-0.089930	4.818078
458.517255	8000.361482	9.916570	-0.089949	4.818113
458.358109	8000.077140	9.921575	-0.089919	4.818029
458.473077	8000.264019	9.926579	-0.089941	4.818084
458.597253	8000.275235	9.931584	-0.089964	4.818087
458.606343	8000.038516	9.936589	-0.089966	4.818017
458.727808	8000.225488	9.941594	-0.089988	4.818072
458.893169	8000.221492	9.946599	-0.090019	4.818070
459.273198	8000.457360	9.951603	-0.090090	4.818138
459.238965	8000.352665	9.956608	-0.090084	4.818107
459.142657	8000.318682	9.961613	-0.090066	4.818098
459.232558	8000.436792	9.966618	-0.090083	4.818132
459.097159	8000.388575	9.971623	-0.090057	4.818118
458.750237	8000.115280	9.976627	-0.089993	4.818039
459.028263	8000.302344	9.981632	-0.090044	4.818093
459.211923	8000.339659	9.986637	-0.090079	4.818103
459.239338	8000.406364	9.991642	-0.090084	4.818123
459.425943	8000.380561	9.996647	-0.090119	4.818115
459.345943	8000.462602	10.001651	-0.090104	4.818139
459.531353	8000.478890	10.006656	-0.090138	4.818143
459.126642	8000.234253	10.011661	-0.090063	4.818073
458.918730	8000.379765	10.016666	-0.090024	4.818117
459.251379	8000.349694	10.021671	-0.090086	4.818106
459.320028	8000.207494	10.026675	-0.090099	4.818064
459.704349	8000.519220	10.031680	-0.090171	4.818155
459.653211	8000.454289	10.036685	-0.090161	4.818136
459.566075	8000.419380	10.041690	-0.090145	4.818126
459.420781	8000.368919	10.046695	-0.090118	4.818111
459.781440	8000.420299	10.051699	-0.090185	4.818125
459.113045	8000.182490	10.056704	-0.090060	4.818057
459.368211	8000.269232	10.061709	-0.090108	4.818082
459.328042	8000.363411	10.066714	-0.090100	4.818110
459.464189	8000.292686	10.071719	-0.090126	4.818088
459.734691	8000.443860	10.076723	-0.090176	4.818132
459.485168	8000.471940	10.081728	-0.090130	4.818142
459.873241	8000.340537	10.086733	-0.090202	4.818101
459.718627	8000.407846	10.091738	-0.090173	4.818122
459.476235	8000.329704	10.096743	-0.090128	4.818099
459.626223	8000.361285	10.101747	-0.090156	4.818108
459.592226	8000.309227	10.106752	-0.090150	4.818093
459.754832	8000.433623	10.111757	-0.090180	4.818129
459.434309	8000.447021	10.116762	-0.090120	4.818134
459.911894	8000.445304	10.121767	-0.090209	4.818132
459.644216	8000.345752	10.126771	-0.090160	4.818103
459.442310	8000.347131	10.131776	-0.090122	4.818105
459.934041	8000.360348	10.136781	-0.090214	4.818107
459.881666	8000.529100	10.141786	-0.090204	4.818157
459.736182	8000.428104	10.146791	-0.090177	4.818128
459.516523	8000.247118	10.151795	-0.090136	4.818075
459.178004	8000.267635	10.156800	-0.090073	4.818082
458.574352	7999.945479	10.161805	-0.089960	4.817989
458.936305	8000.195823	10.166810	-0.090028	4.818062
458.964085	8000.098316	10.171815	-0.090033	4.818033
459.547320	8000.135971	10.176819	-0.090141	4.818042
459.081176	8000.272597	10.181824	-0.090055	4.818084
459.687696	8000.364270	10.186829	-0.090168	4.818109
459.581184	8000.221716	10.191834	-0.090148	4.818067
459.548423	8000.265470	10.196839	-0.090142	4.818080
459.776811	8000.352891	10.201843	-0.090184	4.818105
459.914510	8000.452726	10.206848	-0.090210	4.818134
459.552049	8000.112885	10.211853	-0.090142	4.818035
459.766436	8000.458018	10.216858	-0.090183	4.818136
459.471578	8000.234922	10.221863	-0.090128	4.818071
459.833918	8000.314748	10.226867	-0.090195	4.818093
459.958634	8000.336500	10.231872	-0.090218	4.818099
459.986819	8000.467432	10.236877	-0.090224	4.818138
460.176321	8000.512202	10.241882	-0.090259	4.818151
459.653986	8000.340649	10.246887	-0.090162	4.818102
459.642789	8000.121535	10.251891	-0.090159	4.818037
459.910588	8000.326356	10.256896	-0.090209	4.818097
460.012030	8000.365678	10.261901	-0.090228	4.818108
459.592212	8000.335576	10.266906	-0.090150	4.818101
460.225173	8000.252875	10.271911	-0.090268	4.818073
460.359328	8000.422139	10.276915	-0.090293	4.818123
459.930498	8000.391908	10.281920	-0.090213	4.818116
460.228242	8000.364507	10.286925	-0.090269	4.818107
460.361067	8000.524280	10.291930	-0.090294	4.818153
460.224540	8000.439200	10.296935	-0.090268	4.818129
460.350860	8000.376758	10.301939	-0.090292	4.818110
460.340235	8000.338713	10.306944	-0.090290	4.818098
460.300572	8000.378160	10.311949	-0.090282	4.818110
460.089342	8000.423620	10.316954	-0.090243	4.818125
459.740099	8000.199759	10.321959	-0.090178	4.818060
459.893201	8000.299809	10.326963	-0.090206	4.818089
459.643293	8000.198403	10.331968	-0.090160	4.818060
460.267293	8000.340853	10.336973	-0.090276	4.818099
460.078733	8000.436109	10.341978	-0.090241	4.818128
459.982094	8000.092627	10.346983	-0.090223	4.818027
460.060491	8000.353744	10.351987	-0.090238	4.818104
460.230466	8000.408766	10.356992	-0.090269	4.818120
460.228299	8000.244514	10.361997	-0.090269	4.818071
460.098979	8000.345865	10.367002	-0.090245	4.818102
460.148414	8000.288661	10.372007	-0.090254	4.818084
459.941699	8000.286814	10.377011	-0.090216	4.818085
459.920043	8000.226508	10.382016	-0.090211	4.818067
459.984068	8000.177930	10.387021	-0.090223	4.818052
459.688420	8000.030619	10.392026	-0.090168	4.818010
460.000746	8000.223432	10.397031	-0.090227	4.818066
460.248608	8000.345867	10.402035	-0.090273	4.818101
460.326227	8000.410120	10.407040	-0.090287	4.818120
460.269806	8000.387222	10.412045	-0.090277	4.818113
460.086965	8000.405711	10.417050	-0.090243	4.818119
460.228988	8000.332963	10.422055	-0.090269	4.818097
460.510752	8000.440085	10.427059	-0.090322	4.818128
460.406777	8000.440732	10.432064	-0.090302	4.818128
460.391094	8000.365770	10.437069	-0.090299	4.818106
460.301767	8000.432943	10.442074	-0.090283	4.818127
460.504811	8000.366316	10.447079	-0.090321	4.818106
460.292322	8000.262274	10.452083	-0.090281	4.818076
460.399557	8000.428003	10.457088	-0.090301	4.818125
460.636233	8000.348162	10.462093	-0.090345	4.818100
460.627464	8000.513317	10.467098	-0.090344	4.818149
460.352478	8000.421028	10.472103	-0.090292	4.818123
460.607489	8000.431979	10.477107	-0.090340	4.818125
460.633604	8000.480772	10.482112	-0.090345	4.818139
460.123356	8000.298859	10.487117	-0.090250	4.818088
460.376939	8000.388742	10.492122	-0.090297	4.818113
460.016133	8000.189981	10.497127	-0.090230	4.818056
460.247023	8000.385867	10.502131	-0.090273	4.818113
459.563064	8000.028884	10.507136	-0.090145	4.818010
459.583138	7999.857582	10.512141	-0.090149	4.817959
460.155621	8000.018249	10.517146	-0.090256	4.818004
459.876463	8000.144866	10.522151	-0.090204	4.818043
460.358124	8000.310584	10.527155	-0.090293	4.818090
460.426786	8000.478930	10.532160	-0.090306	4.818140
460.338388	8000.206091	10.537165	-0.090290	4.818059
460.316795	8000.397381	10.542170	-0.090286	4.818116
460.273911	8000.324143	10.547175	-0.090278	4.818094
460.123700	8000.271506	10.552179	-0.090250	4.818079
460.178631	8000.365969	10.557184	-0.090260	4.818107
460.144606	8000.231799	10.562189	-0.090254	4.818068
459.845539	8000.163390	10.567194	-0.090198	4.818049
460.231617	8000.242497	10.572199	-0.090270	4.818070
460.616944	8000.446869	10.577203	-0.090342	4.818129
460.693973	8000.410054	10.582208	-0.090356	4.818118
460.638531	8000.481914	10.587213	-0.090346	4.818140
460.383712	8000.436228	10.592218	-0.090298	4.818127
460.323746	8000.333274	10.597223	-0.090287	4.818097
460.486710	8000.430307	10.602227	-0.090318	4.818125
460.582102	8000.431648	10.607232	-0.090335	4.818125
460.799597	8000.472601	10.612237	-0.090376	4.818136
460.644029	8000.393569	10.617242	-0.090347	4.818113
460.514295	8000.388590	10.622247	-0.090323	4.818113
460.933655	8000.450274	10.627251	-0.090401	4.818129
460.685479	8000.362572	10.632256	-0.090355	4.818104
460.589159	8000.451754	10.637261	-0.090337	4.818131
460.568281	8000.438830	10.642266	-0.090333	4.818127
460.439962	8000.433871	10.647271	-0.090309	4.818126
460.538565	8000.371040	10.652275	-0.090327	4.818107
460.136288	8000.224332	10.657280	-0.090252	4.818065
460.124990	8000.064166	10.662285	-0.090250	4.818018
460.654539	8000.485313	10.667290	-0.090349	4.818141
460.655607	8000.414796	10.672295	-0.090349	4.818120
460.271530	8000.337821	10.677299	-0.090278	4.818098
460.394967	8000.245863	10.682304	-0.090301	4.818071
460.311246	8000.238373	10.687309	-0.090285	4.818069
460.363844	8000.385439	10.692314	-0.090295	4.818112
460.621583	8000.320632	10.697319	-0.090343	4.818092
460.156169	8000.263570	10.702323	-0.090256	4.818077
459.901153	8000.318943	10.707328	-0.090209	4.818094
460.486983	8000.169261	10.712333	-0.090318	4.818048
460.683731	8000.374144	10.717338	-0.090355	4.818108
460.094653	8000.259552	10.722343	-0.090245	4.818076
460.510724	8000.347504	10.727347	-0.090322	4.818100
460.507423	8000.252715	10.732352	-0.090322	4.818072
460.349798	8000.327351	10.737357	-0.090292	4.818095
460.321966	8000.310118	10.742362	-0.090287	4.818090
460.411426	8000.239791	10.747367	-0.090304	4.818069
460.849176	8000.301730	10.752371	-0.090385	4.818085
460.717907	8000.211461	10.757376	-0.090361	4.818059
460.813706	8000.261231	10.762381	-0.090379	4.818073
460.814067	8000.198074	10.767386	-0.090379	4.818055
460.716696	8000.303033	10.772391	-0.090361	4.818086
460.461783	8000.119443	10.777395	-0.090313	4.818033
460.386423	8000.193128	10.782400	-0.090299	4.818055
460.131429	8000.167444	10.787405	-0.090252	4.818049
460.360650	8000.286459	10.792410	-0.090295	4.818083
460.611385	8000.321561	10.797415	-0.090341	4.818092
460.454602	8000.335151	10.802419	-0.090312	4.818097
460.681072	8000.252009	10.807424	-0.090354	4.818071
460.520357	8000.356078	10.812429	-0.090324	4.818103
461.102112	8000.427411	10.817434	-0.090433	4.818122
461.105666	8000.440095	10.822439	-0.090433	4.818125
460.921607	8000.237493	10.827443	-0.090399	4.818066
460.648631	8000.484209	10.832448	-0.090348	4.818140
461.048002	8000.343490	10.837453	-0.090423	4.818097
461.003393	8000.478666	10.842458	-0.090415	4.818137
461.070416	8000.366966	10.847463	-0.090427	4.818104
461.033589	8000.449616	10.852467	-0.090420	4.818128
460.671372	8000.324520	10.857472	-0.090353	4.818093
460.876855	8000.249505	10.862477	-0.090391	4.818070
460.901991	8000.458298	10.867482	-0.090396	4.818132
460.661921	8000.420188	10.872487	-0.090351	4.818121
460.704479	8000.381835	10.877491	-0.090359	4.818110
460.635714	8000.322972	10.882496	-0.090346	4.818093
460.778734	8000.279714	10.887501	-0.090373	4.818079
460.653686	8000.343227	10.892506	-0.090349	4.818098
460.915530	8000.333219	10.897511	-0.090398	4.818094
460.735888	8000.350700	10.902515	-0.090365	4.818100
460.645477	8000.368380	10.907520	-0.090348	4.818106
461.090969	8000.344108	10.912525	-0.090431	4.818097
460.980490	8000.421512	10.917530	-0.090410	4.818120
461.085017	8000.342973	10.922535	-0.090430	4.818097
460.789761	8000.368305	10.927539	-0.090375	4.818105
460.935690	8000.272451	10.932544	-0.090402	4.818076
461.018837	8000.209404	10.937549	-0.090417	4.818057
460.348549	8000.183153	10.942554	-0.090293	4.818052
460.457366	8000.001512	10.947559	-0.090313	4.817998
460.918809	8000.390123	10.952563	-0.090399	4.818111
460.699745	8000.278618	10.957568	-0.090358	4.818079
460.765614	8000.092162	10.962573	-0.090370	4.818024
460.778551	8000.133400	10.967578	-0.090373	4.818036
461.132359	8000.405759	10.972583	-0.090439	4.818115
461.289074	8000.386906	10.977587	-0.090468	4.818109
461.358531	8000.387883	10.982592	-0.090481	4.818109
461.261809	8000.322308	10.987597	-0.090463	4.818090
461.328623	8000.434838	10.992602	-0.090475	4.818123
461.101251	8000.331636	10.997607	-0.090433	4.818093
461.506197	8000.364695	11.002611	-0.090508	4.818101
461.416879	8000.519247	11.007616	-0.090492	4.818147
461.359435	8000.264731	11.012621	-0.090481	4.818072
461.165248	8000.380964	11.017626	-0.090445	4.818108
461.030250	8000.203264	11.022631	-0.090420	4.818055
461.228153	8000.302895	11.027635	-0.090457	4.818084
461.356162	8000.446813	11.032640	-0.090481	4.818126
461.182672	8000.263307	11.037645	-0.090448	4.818073
461.292435	8000.455394	11.042650	-0.090469	4.818129
461.011704	8000.357759	11.047655	-0.090417	4.818101
461.119954	8000.263482	11.052659	-0.090437	4.818073
460.915237	8000.394305	11.057664	-0.090399	4.818113
460.817213	7999.997109	11.062669	-0.090380	4.817995
460.355854	8000.039061	11.067674	-0.090294	4.818009
460.601893	8000.023566	11.072679	-0.090340	4.818004
460.807710	8000.032771	11.077683	-0.090378	4.818006
460.717180	8000.264149	11.082688	-0.090362	4.818075
461.034840	8000.145442	11.087693	-0.090421	4.818038
461.041420	8000.401347	11.092698	-0.090422	4.818114
461.159932	8000.324058	11.097703	-0.090444	4.818091
461.071027	8000.300703	11.102707	-0.090428	4.818084
460.856780	8000.339805	11.107712	-0.090388	4.818097
460.935655	8000.359862	11.112717	-0.090403	4.818102
460.724552	8000.204255	11.117722	-0.090363	4.818057
460.692715	8000.178544	11.122727	-0.090357	4.818049
460.892966	8000.296102	11.127731	-0.090395	4.818083
460.227510	8000.012009	11.132736	-0.090271	4.818002
460.715123	7999.989375	11.137741	-0.090361	4.817993
460.554825	8000.258724	11.142746	-0.090332	4.818074
460.740434	8000.098161	11.147751	-0.090366	4.818025
461.398196	8000.400053	11.152755	-0.090489	4.818112
460.989637	8000.266936	11.157760	-0.090413	4.818074
461.196262	8000.269839	11.162765	-0.090451	4.818074
461.268384	8000.347702	11.167770	-0.090465	4.818097
461.414314	8000.281324	11.172775	-0.090492	4.818077
461.406776	8000.379124	11.177779	-0.090490	4.818106
460.913648	8000.365883	11.182784	-0.090399	4.818104
461.107389	8000.247541	11.187789	-0.090435	4.818068
461.371689	8000.389161	11.192794	-0.090484	4.818109
461.235191	8000.370401	11.197799	-0.090459	4.818104
461.245773	8000.306334	11.202803	-0.090460	4.818085
461.270395	8000.362476	11.207808	-0.090465	4.818102
461.147991	8000.254432	11.212813	-0.090442	4.818070
461.370976	8000.298621	11.217818	-0.090484	4.818082
461.133746	8000.317398	11.222823	-0.090440	4.818089
460.843113	8000.099617	11.227827	-0.090385	4.818025
461.263290	8000.391858	11.232832	-0.090464	4.818110
461.553716	8000.404360	11.237837	-0.090518	4.818113
461.284149	8000.455317	11.242842	-0.090468	4.818129
461.592479	8000.322792	11.247847	-0.090525	4.818088
461.914877	8000.482077	11.252851	-0.090585	4.818134
462.223955	8000.420097	11.257856	-0.090643	4.818115
461.899273	8000.529233	11.262861	-0.090582	4.818148
461.798801	8000.457288	11.267866	-0.090564	4.818128
461.838479	8000.433633	11.272871	-0.090571	4.818120
462.000471	8000.433805	11.277875	-0.090601	4.818120
461.701220	8000.432759	11.282880	-0.090546	4.818121
461.736396	8000.347982	11.287885	-0.090552	4.818095
461.743324	8000.474410	11.292890	-0.090553	4.818133
461.517280	8000.411229	11.297895	-0.090511	4.818115
461.228308	8000.392433	11.302899	-0.090458	4.818111
461.057987	8000.306876	11.307904	-0.090426	4.818086
461.009964	8000.070394	11.312909	-0.090417	4.818016
460.972039	8000.197241	11.317914	-0.090410	4.818054
461.267513	8000.129805	11.322919	-0.090465	4.818033
461.607608	8000.128265	11.327923	-0.090528	4.818031
460.874330	8000.014807	11.332928	-0.090391	4.818000
461.091714	8000.147342	11.337933	-0.090432	4.818039
461.614288	8000.255742	11.342938	-0.090529	4.818068
461.300962	8000.323981	11.347943	-0.090471	4.818090
461.315486	8000.151539	11.352947	-0.090474	4.818039
461.095560	8000.301097	11.357952	-0.090433	4.818084
461.378829	8000.142956	11.362957	-0.090486	4.818036
461.435140	8000.366926	11.367962	-0.090496	4.818102
461.444985	8000.303902	11.372967	-0.090498	4.818083
461.519135	8000.446011	11.377971	-0.090512	4.818125
461.081371	8000.333537	11.382976	-0.090430	4.818094
461.511864	8000.253260	11.387981	-0.090510	4.818068
461.412632	8000.276080	11.392986	-0.090492	4.818075
461.785081	8000.357109	11.397991	-0.090561	4.818098
461.931394	8000.436017	11.402995	-0.090589	4.818121
461.727389	8000.393147	11.408000	-0.090551	4.818109
461.968933	8000.359695	11.413005	-0.090596	4.818098
462.048739	8000.517678	11.418010	-0.090611	4.818144
461.914756	8000.424207	11.423015	-0.090586	4.818117
461.624857	8000.266434	11.428019	-0.090532	4.818072
461.274413	8000.325731	11.433024	-0.090466	4.818091
461.368448	8000.085978	11.438029	-0.090484	4.818019
461.580866	8000.350039	11.443034	-0.090524	4.818097
461.662316	8000.457511	11.448039	-0.090539	4.818128
461.388370	8000.292595	11.453043	-0.090488	4.818080
461.883667	8000.424829	11.458048	-0.090580	4.818118
461.729231	8000.381603	11.463053	-0.090551	4.818105
461.606843	8000.493582	11.468058	-0.090529	4.818139
461.489568	8000.357184	11.473063	-0.090507	4.818099
461.517215	8000.372312	11.478067	-0.090512	4.818103
461.434253	8000.477474	11.483072	-0.090496	4.818135
461.403470	8000.090690	11.488077	-0.090490	4.818020
461.152463	8000.288237	11.493082	-0.090444	4.818080
461.436258	8000.383811	11.498087	-0.090497	4.818107
461.638760	8000.337178	11.503091	-0.090534	4.818093
461.685654	8000.467325	11.508096	-0.090543	4.818131
461.681557	8000.330412	11.513101	-0.090542	4.818090
461.704031	8000.446531	11.518106	-0.090547	4.818125
461.900077	8000.522979	11.523111	-0.090583	4.818147
461.791400	8000.355118	11.528115	-0.090563	4.818097
461.726807	8000.421588	11.533120	-0.090551	4.818117
461.871375	8000.429936	11.538125	-0.090578	4.818119
461.840369	8000.466348	11.543130	-0.090572	4.818130
461.602714	8000.321942	11.548135	-0.090528	4.818088
461.788707	8000.381404	11.553139	-0.090563	4.818105
462.042109	8000.522876	11.558144	-0.090610	4.818146
462.293992	8000.334814	11.563149	-0.090657	4.818089
461.957342	8000.464838	11.568154	-0.090594	4.818129
462.116563	8000.478657	11.573159	-0.090624	4.818133
462.163226	8000.360352	11.578163	-0.090632	4.818097
462.056301	8000.470443	11.583168	-0.090612	4.818130
462.022223	8000.321526	11.588173	-0.090606	4.818086
462.064665	8000.421082	11.593178	-0.090614	4.818116
462.132978	8000.434676	11.598183	-0.090627	4.818119
461.951302	8000.344746	11.603187	-0.090593	4.818093
461.878399	8000.450051	11.608192	-0.090579	4.818125
461.953657	8000.305829	11.613197	-0.090593	4.818082
461.814495	8000.284926	11.618202	-0.090567	4.818076
461.808117	8000.111136	11.623207	-0.090566	4.818025
462.222510	8000.364353	11.628211	-0.090643	4.818098
461.835297	8000.359966	11.633216	-0.090571	4.818098
461.677999	8000.206163	11.638221	-0.090542	4.818054
462.017965	8000.376220	11.643226	-0.090605	4.818103
461.860745	8000.275054	11.648231	-0.090576	4.818073
461.855240	8000.121278	11.653235	-0.090575	4.818028
462.111124	8000.407009	11.658240	-0.090623	4.818111
462.241287	8000.264612	11.663245	-0.090647	4.818068
462.236032	8000.368761	11.668250	-0.090646	4.818099
461.884138	8000.333289	11.673255	-0.090581	4.818090
462.145757	8000.312752	11.678259	-0.090629	4.818083
461.965962	8000.403922	11.683264	-0.090596	4.818111
461.904828	8000.215675	11.688269	-0.090584	4.818055
461.954235	8000.376387	11.693274	-0.090594	4.818103
461.899042	8000.361927	11.698279	-0.090583	4.818099
462.022167	8000.239434	11.703283	-0.090606	4.818062
461.679123	8000.325152	11.708288	-0.090542	4.818089
461.590069	8000.104934	11.713293	-0.090526	4.818024
461.830653	8000.255696	11.718298	-0.090571	4.818068
461.737537	8000.357558	11.723303	-0.090553	4.818098
461.358004	8000.090099	11.728307	-0.090483	4.818020
461.101928	8000.059135	11.733312	-0.090435	4.818012
461.017250	8000.070580	11.738317	-0.090419	4.818016
461.368719	8000.082883	11.743322	-0.090485	4.818018
461.168215	7999.997958	11.748327	-0.090447	4.817994
461.675907	8000.061932	11.753331	-0.090542	4.818011
461.612446	8000.298960	11.758336	-0.090530	4.818081
461.683895	8000.165214	11.763341	-0.090543	4.818041
461.510627	8000.128042	11.768346	-0.090511	4.818031
461.255647	8000.158150	11.773351	-0.090464	4.818041
461.361315	7999.858559	11.778355	-0.090483	4.817952
461.573272	8000.179455	11.783360	-0.090523	4.818046
461.543820	8000.115879	11.788365	-0.090517	4.818027
461.471408	8000.021171	11.793370	-0.090504	4.818000
461.540921	8000.141106	11.798375	-0.090517	4.818035
461.409680	7999.967671	11.803379	-0.090492	4.817984
461.158766	8000.018891	11.808384	-0.090446	4.818000
461.278903	7999.806879	11.813389	-0.090468	4.817937
461.587562	8000.223878	11.818394	-0.090526	4.818059
460.953938	7999.991808	11.823399	-0.090408	4.817993
461.228267	7999.917758	11.828403	-0.090459	4.817970
461.246592	7999.991706	11.833408	-0.090462	4.817992
461.186346	7999.819271	11.838413	-0.090451	4.817941
460.985903	7999.896464	11.843418	-0.090413	4.817965
461.110663	7999.920323	11.848423	-0.090437	4.817971
461.154133	7999.906196	11.853427	-0.090445	4.817967
461.276904	8000.108987	11.858432	-0.090468	4.818026
461.379639	8000.093587	11.863437	-0.090487	4.818021
461.033071	7999.943450	11.868442	-0.090422	4.817978
461.345817	8000.091009	11.873447	-0.090481	4.818021
460.984999	7999.880668	11.878451	-0.090413	4.817960
461.331776	8000.036072	11.883456	-0.090478	4.818004
461.066389	7999.820756	11.888461	-0.090429	4.817942
460.668740	7999.908867	11.893466	-0.090355	4.817970
460.674162	7999.941578	11.898471	-0.090356	4.817979
461.144970	7999.810281	11.903475	-0.090443	4.817938
460.971888	7999.899439	11.908480	-0.090411	4.817965
461.255782	7999.802364	11.913485	-0.090464	4.817936
461.146912	7999.929267	11.918490	-0.090444	4.817974
460.841622	7999.812346	11.923495	-0.090387	4.817940
460.980384	7999.802714	11.928499	-0.090413	4.817937
461.132171	7999.994330	11.933504	-0.090441	4.817993
461.326379	7999.937053	11.938509	-0.090477	4.817975
461.250211	8000.211796	11.943514	-0.090463	4.818057
461.599329	8000.207225	11.948519	-0.090528	4.818054
461.715278	8000.068841	11.953523	-0.090550	4.818013
461.600370	8000.109337	11.958528	-0.090528	4.818025
461.726797	8000.076373	11.963533	-0.090552	4.818015
461.997119	8000.159125	11.968538	-0.090602	4.818038
462.015496	8000.307821	11.973543	-0.090606	4.818082
461.734757	7999.988059	11.978547	-0.090553	4.817989
461.354284	7999.989036	11.983552	-0.090483	4.817990
461.086795	7999.850537	11.988557	-0.090433	4.817950
461.237248	7999.824226	11.993562	-0.090461	4.817942
461.127594	7999.920589	11.998567	-0.090440	4.817971
461.371012	7999.935586	12.003571	-0.090486	4.817975
461.041600	7999.854117	12.008576	-0.090424	4.817952
461.157794	7999.945228	12.013581	-0.090446	4.817978
461.851931	8000.093932	12.018586	-0.090575	4.818019
461.211919	7999.920725	12.023591	-0.090456	4.817971
461.138470	7999.837585	12.028595	-0.090442	4.817946
461.576839	8000.066913	12.033600	-0.090524	4.818013
461.442845	7999.901862	12.038605	-0.090499	4.817964
461.482862	7999.930848	12.043610	-0.090507	4.817973
461.489098	8000.060420	12.048615	-0.090508	4.818011
461.148162	7999.813514	12.053619	-0.090444	4.817939
461.177117	7999.993933	12.058624	-0.090450	4.817993
461.361311	7999.938620	12.063629	-0.090484	4.817975
461.697595	7999.992819	12.068634	-0.090547	4.817990
461.443422	8000.061889	12.073639	-0.090499	4.818012
461.628147	8000.139227	12.078643	-0.090534	4.818034
461.341224	8000.074142	12.083648	-0.090480	4.818016
461.764132	7999.885327	12.088653	-0.090559	4.817958
461.930974	8000.071897	12.093658	-0.090590	4.818013
461.248554	7999.933886	12.098663	-0.090463	4.817975
461.521035	8000.013507	12.103667	-0.090514	4.817997
461.885364	8000.303914	12.108672	-0.090582	4.818082
461.967809	8000.201904	12.113677	-0.090597	4.818051
461.845748	8000.220193	12.118682	-0.090575	4.818057
461.277157	7999.925871	12.123687	-0.090468	4.817972
461.747683	8000.129335	12.128691	-0.090556	4.818030
461.374335	8000.100934	12.133696	-0.090487	4.818024
461.479151	8000.119251	12.138701	-0.090506	4.818029
461.437591	8000.087086	12.143706	-0.090498	4.818019
461.828441	8000.285226	12.148711	-0.090571	4.818076
462.068476	8000.113843	12.153715	-0.090616	4.818024
461.637961	8000.145697	12.158720	-0.090536	4.818036
462.298316	8000.290777	12.163725	-0.090659	4.818076
462.501553	8000.348377	12.168730	-0.090697	4.818092
462.312078	8000.330977	12.173735	-0.090662	4.818088
461.951395	8000.186948	12.178739	-0.090594	4.818047
462.130292	8000.327372	12.183744	-0.090628	4.818088
462.172446	8000.210057	12.188749	-0.090636	4.818053
462.368590	8000.243343	12.193754	-0.090672	4.818062
462.356978	8000.442153	12.198759	-0.090670	4.818121
462.822826	8000.440279	12.203763	-0.090757	4.818118
462.606608	8000.428819	12.208768	-0.090717	4.818116
462.470237	8000.463750	12.213773	-0.090691	4.818127
462.170489	8000.185822	12.218778	-0.090635	4.818045
462.382249	8000.263543	12.223783	-0.090675	4.818068
462.476601	8000.337510	12.228787	-0.090692	4.818089
462.408736	8000.380774	12.233792	-0.090680	4.818102
462.779187	8000.403878	12.238797	-0.090749	4.818108
462.858922	8000.417633	12.243802	-0.090764	4.818111
462.348525	8000.383089	12.248807	-0.090669	4.818103
462.018676	7999.977361	12.253811	-0.090607	4.817984
462.028049	8000.258574	12.258816	-0.090609	4.818068
462.057421	8000.185296	12.263821	-0.090614	4.818046
462.029579	8000.065946	12.268826	-0.090609	4.818010
462.242201	8000.286852	12.273831	-0.090649	4.818075
462.698820	8000.212206	12.278835	-0.090734	4.818051
462.825380	8000.500339	12.283840	-0.090758	4.818136
462.768811	8000.310045	12.288845	-0.090747	4.818080
462.740720	8000.337023	12.293850	-0.090742	4.818088
462.243236	8000.265816	12.298855	-0.090649	4.818069
462.628196	8000.410191	12.303859	-0.090721	4.818110
462.711335	8000.394516	12.308864	-0.090736	4.818105
462.457238	8000.366732	12.313869	-0.090689	4.818098
462.252006	8000.255416	12.318874	-0.090651	4.818066
462.508478	8000.343241	12.323879	-0.090699	4.818091
462.440262	8000.202266	12.328883	-0.090686	4.818049
462.284997	8000.335891	12.333888	-0.090657	4.818089
462.295178	8000.266553	12.338893	-0.090659	4.818069
462.239454	8000.254191	12.343898	-0.090648	4.818065
461.874317	8000.035358	12.348903	-0.090580	4.818002
462.154049	8000.019285	12.353907	-0.090632	4.817996
462.632047	8000.393411	12.358912	-0.090722	4.818105
462.478707	8000.396521	12.363917	-0.090693	4.818107
462.706016	8000.328128	12.368922	-0.090735	4.818085
462.577520	8000.313690	12.373927	-0.090711	4.818082
462.734253	8000.544346	12.378931	-0.090741	4.818149
462.707263	8000.391315	12.383936	-0.090736	4.818104
462.599448	8000.321371	12.388941	-0.090716	4.818084
462.987226	8000.394199	12.393946	-0.090788	4.818104
462.949805	8000.496847	12.398951	-0.090781	4.818134
463.147351	8000.429088	12.403955	-0.090818	4.818113
462.978204	8000.471981	12.408960	-0.090786	4.818127
462.707964	8000.251313	12.413965	-0.090736	4.818063
462.797982	8000.455763	12.418970	-0.090753	4.818123
462.651781	8000.380015	12.423975	-0.090725	4.818101
462.788695	8000.299824	12.428979	-0.090751	4.818077
462.748541	8000.449807	12.433984	-0.090744	4.818121
462.591508	8000.265473	12.438989	-0.090714	4.818067
462.488738	8000.191389	12.443994	-0.090695	4.818046
462.660240	8000.319079	12.448999	-0.090727	4.818083
462.373445	8000.217143	12.454003	-0.090674	4.818054
462.515720	8000.371793	12.459008	-0.090700	4.818099
462.376624	8000.182449	12.464013	-0.090674	4.818044
462.254103	8000.212312	12.469018	-0.090651	4.818053
462.282867	8000.177976	12.474023	-0.090657	4.818043
462.096191	8000.139562	12.479027	-0.090622	4.818032
462.246883	8000.179578	12.484032	-0.090650	4.818043
462.273547	8000.071521	12.489037	-0.090655	4.818011
461.811795	7999.986083	12.494042	-0.090569	4.817988
461.709196	8000.087811	12.499047	-0.090550	4.818018
461.692840	7999.830719	12.504051	-0.090547	4.817942
462.439741	8000.233877	12.509056	-0.090686	4.818059
462.362912	8000.263328	12.514061	-0.090672	4.818068
462.129080	8000.284257	12.519066	-0.090628	4.818075
462.012171	8000.193133	12.524071	-0.090607	4.818048
462.212068	8000.156990	12.529075	-0.090644	4.818037
462.272841	8000.258909	12.534080	-0.090655	4.818067
462.331599	8000.322900	12.539085	-0.090666	4.818085
462.537838	8000.391071	12.544090	-0.090705	4.818105
462.296907	8000.269777	12.549095	-0.090660	4.818070
462.781675	8000.176577	12.554099	-0.090750	4.818040
462.477953	8000.255479	12.559104	-0.090693	4.818065
462.510918	8000.128559	12.564109	-0.090699	4.818027
462.232429	8000.183602	12.569114	-0.090648	4.818044
462.510812	8000.193831	12.574119	-0.090700	4.818046
462.578870	8000.190577	12.579123	-0.090712	4.818045
462.440128	8000.319170	12.584128	-0.090686	4.818084
462.531946	8000.188867	12.589133	-0.090703	4.818045
462.676458	8000.393029	12.594138	-0.090731	4.818105
462.430486	8000.349568	12.599143	-0.090685	4.818093
462.340032	8000.125114	12.604147	-0.090668	4.818027
462.144170	8000.210795	12.609152	-0.090631	4.818053
462.267225	8000.108302	12.614157	-0.090654	4.818022
461.946614	8000.206969	12.619162	-0.090595	4.818053
462.311126	8000.370003	12.624167	-0.090663	4.818099
462.240563	8000.211100	12.629171	-0.090649	4.818053
462.036422	8000.147174	12.634176	-0.090611	4.818034
462.071660	7999.909753	12.639181	-0.090618	4.817964
461.607651	7999.885344	12.644186	-0.090531	4.817959
461.557296	7999.836214	12.649191	-0.090522	4.817944
461.939134	7999.839468	12.654195	-0.090593	4.817944
461.934328	8000.009943	12.659200	-0.090592	4.817994
462.206077	8000.044289	12.664205	-0.090643	4.818003
461.722310	8000.051183	12.669210	-0.090553	4.818007
462.272164	8000.105225	12.674215	-0.090655	4.818021
462.472052	8000.101717	12.679219	-0.090693	4.818019
462.069876	8000.076068	12.684224	-0.090618	4.818013
462.003006	8000.059339	12.689229	-0.090605	4.818009
462.337203	8000.186151	12.694234	-0.090667	4.818045
462.377629	8000.307787	12.699239	-0.090675	4.818081
462.206737	8000.055886	12.704243	-0.090643	4.818007
462.171832	8000.038553	12.709248	-0.090637	4.818002
462.454550	8000.067790	12.714253	-0.090689	4.818009
462.314003	7999.978440	12.719258	-0.090663	4.817983
461.747295	7999.969432	12.724263	-0.090558	4.817983
461.474500	7999.835068	12.729267	-0.090507	4.817944
461.413064	7999.942635	12.734272	-0.090495	4.817976
461.824338	7999.978938	12.739277	-0.090572	4.817985
462.008324	7999.893093	12.744282	-0.090606	4.817959
462.156489	8000.101510	12.749287	-0.090634	4.818020
461.709961	7999.947859	12.754291	-0.090551	4.817977
461.304801	7999.846377	12.759296	-0.090475	4.817948
461.540451	7999.820209	12.764301	-0.090519	4.817940
461.422126	7999.849078	12.769306	-0.090497	4.817949
461.406195	7999.829907	12.774311	-0.090494	4.817943
461.010451	7999.867516	12.779315	-0.090420	4.817956
460.982436	7999.782908	12.784320	-0.090415	4.817931
461.727513	7999.823892	12.789325	-0.090554	4.817940
461.914076	7999.974945	12.794330	-0.090589	4.817984
461.897072	7999.992604	12.799335	-0.090586	4.817989
461.796051	7999.928023	12.804339	-0.090567	4.817970
461.362324	7999.934569	12.809344	-0.090486	4.817974
461.716194	7999.799526	12.814349	-0.090552	4.817933
461.318378	7999.905531	12.819354	-0.090478	4.817966
461.788341	7999.805804	12.824359	-0.090565	4.817934
462.148329	7999.974030	12.829363	-0.090633	4.817983
462.077664	8000.143582	12.834368	-0.090620	4.818033
461.590083	7999.817762	12.839373	-0.090529	4.817939
461.740167	7999.956723	12.844378	-0.090557	4.817979
462.222166	8000.116137	12.849383	-0.090646	4.818024
462.071017	8000.106646	12.854387	-0.090618	4.818022
461.850877	7999.823532	12.859392	-0.090577	4.817939
461.921697	7999.974013	12.864397	-0.090590	4.817984
461.784800	7999.829975	12.869402	-0.090565	4.817941
461.761258	7999.964394	12.874407	-0.090561	4.817981
462.179539	7999.945001	12.879411	-0.090638	4.817974
462.157128	7999.905737	12.884416	-0.090634	4.817962
462.169806	7999.916443	12.889421	-0.090637	4.817965
462.297607	7999.969822	12.894426	-0.090660	4.817981
462.291499	8000.003425	12.899431	-0.090659	4.817991
462.239582	7999.861631	12.904435	-0.090650	4.817949
462.027276	8000.019719	12.909440	-0.090610	4.817997
462.342385	7999.926240	12.914445	-0.090669	4.817968
462.150447	7999.968814	12.919450	-0.090633	4.817981
461.921402	8000.134036	12.924455	-0.090591	4.818031
461.932607	7999.832062	12.929459	-0.090593	4.817941
461.762664	7999.892840	12.934464	-0.090561	4.817960
461.653697	7999.882890	12.939469	-0.090541	4.817958
462.161297	8000.107932	12.944474	-0.090635	4.818022
461.702515	7999.802518	12.949479	-0.090550	4.817934
462.023345	7999.811233	12.954483	-0.090609	4.817935
461.683973	7999.850685	12.959488	-0.090546	4.817948
461.788419	7999.855310	12.964493	-0.090566	4.817949
461.699464	7999.816165	12.969498	-0.090549	4.817938
461.632398	7999.945761	12.974503	-0.090537	4.817976
461.911092	7999.762290	12.979507	-0.090589	4.817921
461.862821	7999.851094	12.984512	-0.090580	4.817947
461.340354	7999.821656	12.989517	-0.090482	4.817941
461.219872	7999.823125	12.994522	-0.090460	4.817942
462.034310	7999.897719	12.999527	-0.090612	4.817960
461.665992	7999.764119	13.004531	-0.090543	4.817922
461.647876	8000.024939	13.009536	-0.090540	4.818000
461.461564	7999.747567	13.014541	-0.090505	4.817918
461.822902	7999.964235	13.019546	-0.090572	4.817981
461.600829	7999.859005	13.024551	-0.090531	4.817951
461.834043	7999.840172	13.029555	-0.090574	4.817944
462.354975	7999.953811	13.034560	-0.090672	4.817976
462.337877	8000.163068	13.039565	-0.090668	4.818038
462.227483	8000.066771	13.044570	-0.090648	4.818010
462.747210	8000.180401	13.049575	-0.090745	4.818041
462.663167	8000.235017	13.054579	-0.090729	4.818058
462.210912	8000.130759	13.059584	-0.090645	4.818029
462.314630	7999.969042	13.064589	-0.090664	4.817980
462.640620	8000.045207	13.069594	-0.090725	4.818002
462.398588	8000.253411	13.074599	-0.090680	4.818064
462.701148	8000.092381	13.079603	-0.090736	4.818015
462.914743	8000.319621	13.084608	-0.090776	4.818082
462.534258	8000.159520	13.089613	-0.090705	4.818036
461.965598	7999.914669	13.094618	-0.090599	4.817966
461.662022	7999.861984	13.099623	-0.090543	4.817951
461.899655	7999.897954	13.104627	-0.090587	4.817961
462.133333	7999.955978	13.109632	-0.090630	4.817977
462.157139	7999.931047	13.114637	-0.090635	4.817970
462.677556	8000.012048	13.119642	-0.090732	4.817992
462.619918	8000.247056	13.124647	-0.090721	4.818062
462.420549	8000.032654	13.129651	-0.090684	4.817999
462.507669	8000.002296	13.134656	-0.090700	4.817990
462.146080	7999.922475	13.139661	-0.090633	4.817967
462.755240	8000.113155	13.144666	-0.090746	4.818021
462.735619	8000.235001	13.149671	-0.090743	4.818058
462.762898	8000.011148	13.154675	-0.090748	4.817991
462.948103	8000.310630	13.159680	-0.090783	4.818079
462.611427	7999.969018	13.164685	-0.090720	4.817979
462.597765	8000.035150	13.169690	-0.090717	4.817999
462.239010	7999.983793	13.174695	-0.090650	4.817985
462.140324	7999.910822	13.179699	-0.090632	4.817964
461.850248	7999.953071	13.184704	-0.090578	4.817978
461.705014	7999.825760	13.189709	-0.090551	4.817940
461.093306	7999.874023	13.194714	-0.090437	4.817957
462.249795	7999.961841	13.199719	-0.090652	4.817979
462.284983	7999.828640	13.204723	-0.090659	4.817939
462.056248	7999.845432	13.209728	-0.090616	4.817945
462.178200	7999.848197	13.214733	-0.090639	4.817945
462.444277	7999.901412	13.219738	-0.090689	4.817960
462.147842	7999.994102	13.224743	-0.090633	4.817989
462.755556	8000.163709	13.229747	-0.090747	4.818036
462.759147	8000.031113	13.234752	-0.090747	4.817997
462.773337	7999.923933	13.239757	-0.090750	4.817965
463.109211	8000.200264	13.244762	-0.090813	4.818046
462.653021	8000.127531	13.249767	-0.090728	4.818026
462.605195	7999.939472	13.254771	-0.090719	4.817970
462.642101	8000.078953	13.259776	-0.090726	4.818012
462.471719	8000.040768	13.264781	-0.090694	4.818001
462.876268	8000.277006	13.269786	-0.090769	4.818069
462.656145	8000.183376	13.274791	-0.090728	4.818043
462.552061	7999.886094	13.279795	-0.090709	4.817955
462.585890	8000.006582	13.284800	-0.090715	4.817990
462.589544	7999.810825	13.289805	-0.090716	4.817932
462.398397	7999.881833	13.294810	-0.090680	4.817954
462.229262	7999.861563	13.299815	-0.090649	4.817949
462.487589	7999.928355	13.304819	-0.090697	4.817968
462.749127	8000.215219	13.309824	-0.090746	4.818052
463.172210	8000.275910	13.314829	-0.090825	4.818068
463.260507	8000.418225	13.319834	-0.090841	4.818110
462.901809	8000.305800	13.324839	-0.090774	4.818078
462.658998	8000.107629	13.329843	-0.090729	4.818020
461.995533	7999.958298	13.334848	-0.090605	4.817979
462.292988	7999.848780	13.339853	-0.090661	4.817945
462.319975	7999.813368	13.344858	-0.090666	4.817934
462.259968	7999.916746	13.349863	-0.090655	4.817965
462.709839	7999.838845	13.354867	-0.090738	4.817940
462.623249	8000.112396	13.359872	-0.090722	4.818022
462.645954	8000.282210	13.364877	-0.090727	4.818072
462.810939	8000.116087	13.369882	-0.090757	4.818022
462.668246	8000.130928	13.374887	-0.090731	4.818027
463.044399	8000.126739	13.379891	-0.090801	4.818024
462.706958	8000.153582	13.384896	-0.090738	4.818034
462.856763	8000.177795	13.389901	-0.090766	4.818040
462.637430	7999.948374	13.394906	-0.090725	4.817973
462.345683	8000.093767	13.399911	-0.090671	4.818017
462.957119	8000.158153	13.404915	-0.090785	4.818034
462.819585	8000.136219	13.409920	-0.090759	4.818028
462.677257	7999.897353	13.414925	-0.090732	4.817958
462.897005	8000.073091	13.419930	-0.090774	4.818009
463.076516	8000.217737	13.424935	-0.090807	4.818051
463.357868	8000.248011	13.429939	-0.090859	4.818059
463.026479	8000.357054	13.434944	-0.090798	4.818093
463.418207	8000.394146	13.439949	-0.090871	4.818102
463.381894	8000.434695	13.444954	-0.090864	4.818114
462.932638	8000.282044	13.449959	-0.090780	4.818071
463.130406	8000.165862	13.454963	-0.090817	4.818035
463.374111	8000.368263	13.459968	-0.090863	4.818094
463.314083	8000.297936	13.464973	-0.090851	4.818074
462.783470	8000.066242	13.469978	-0.090753	4.818007
462.666206	8000.061437	13.474983	-0.090731	4.818006
462.672242	8000.023624	13.479987	-0.090732	4.817995
462.378648	7999.993183	13.484992	-0.090677	4.817987
462.689118	8000.072289	13.489997	-0.090735	4.818009
462.564579	8000.140023	13.495002	-0.090712	4.818030
462.249081	8000.035582	13.500007	-0.090653	4.818000
462.617547	8000.101817	13.505011	-0.090722	4.818019
462.449642	7999.924704	13.510016	-0.090690	4.817967
462.686967	8000.003836	13.515021	-0.090735	4.817989
462.656442	8000.022357	13.520026	-0.090729	4.817995
462.643560	8000.194829	13.525031	-0.090727	4.818046
462.651766	7999.941232	13.530035	-0.090728	4.817971
462.631773	8000.094653	13.535040	-0.090724	4.818016
463.382306	8000.268379	13.540045	-0.090864	4.818065
462.755545	8000.021649	13.545050	-0.090747	4.817994
462.882084	8000.121333	13.550055	-0.090771	4.818023
463.099519	8000.089648	13.555059	-0.090812	4.818013
462.876065	8000.109670	13.560064	-0.090770	4.818020
462.382654	7999.997466	13.565069	-0.090678	4.817989
462.588619	8000.114056	13.570074	-0.090717	4.818022
462.837642	8000.309158	13.575079	-0.090763	4.818079
462.571398	7999.949588	13.580083	-0.090713	4.817974
462.639266	8000.105296	13.585088	-0.090726	4.818019
462.868149	8000.141148	13.590093	-0.090769	4.818029
462.618366	7999.943934	13.595098	-0.090722	4.817972
462.651478	7999.969666	13.600103	-0.090728	4.817979
463.107741	7999.951862	13.605107	-0.090813	4.817972
462.563001	7999.938949	13.610112	-0.090712	4.817970
462.853902	8000.010411	13.615117	-0.090766	4.817990
462.566394	7999.932682	13.620122	-0.090712	4.817969
462.759402	8000.173315	13.625127	-0.090749	4.818039
462.932130	7999.860970	13.630131	-0.090780	4.817946
463.244193	8000.323307	13.635136	-0.090839	4.818082
462.946511	8000.128573	13.640141	-0.090783	4.818025
462.643929	8000.046419	13.645146	-0.090727	4.818002
462.642536	7999.945337	13.650151	-0.090727	4.817972
462.862694	7999.944219	13.655155	-0.090768	4.817971
462.943476	8000.092740	13.660160	-0.090783	4.818014
463.272208	8000.134207	13.665165	-0.090844	4.818025
463.011648	8000.171604	13.670170	-0.090796	4.818038
462.660966	8000.059297	13.675175	-0.090730	4.818006
463.026968	8000.081284	13.680179	-0.090798	4.818011
463.068582	8000.297687	13.685184	-0.090806	4.818075
463.160886	8000.148439	13.690189	-0.090823	4.818030
463.003138	8000.033578	13.695194	-0.090794	4.817997
463.031466	8000.168730	13.700199	-0.090799	4.818037
463.144928	8000.201909	13.705203	-0.090821	4.818046
463.091852	8000.016930	13.710208	-0.090811	4.817991
463.317630	8000.146435	13.715213	-0.090853	4.818029
462.795088	8000.019080	13.720218	-0.090755	4.817993
462.921094	8000.106124	13.725223	-0.090779	4.818019
462.977656	7999.914266	13.730227	-0.090789	4.817961
463.172900	8000.054920	13.735232	-0.090826	4.818002
462.820832	7999.979441	13.740237	-0.090760	4.817981
462.653677	8000.037101	13.745242	-0.090729	4.817999
462.597934	7999.955258	13.750247	-0.090719	4.817975
463.067556	8000.117663	13.755251	-0.090806	4.818021
463.014007	7999.903202	13.760256	-0.090796	4.817958
462.874799	8000.074952	13.765261	-0.090770	4.818009
463.037499	8000.007756	13.770266	-0.090801	4.817989
462.786415	7999.957910	13.775271	-0.090754	4.817975
462.998668	8000.014582	13.780275	-0.090793	4.817991
463.426161	8000.372217	13.785280	-0.090873	4.818095
462.757024	7999.986977	13.790285	-0.090748	4.817984
462.732453	7999.861356	13.795290	-0.090744	4.817947
462.524769	8000.076358	13.800295	-0.090705	4.818011
462.812100	7999.940379	13.805299	-0.090759	4.817970
462.602708	8000.149042	13.810304	-0.090720	4.818033
462.345127	7999.889609	13.815309	-0.090672	4.817957
462.152877	7999.841644	13.820314	-0.090636	4.817943
462.223078	7999.959483	13.825319	-0.090649	4.817978
463.026681	8000.105523	13.830323	-0.090799	4.818018
463.030164	8000.198216	13.835328	-0.090799	4.818045
462.955734	8000.230859	13.840333	-0.090786	4.818055
463.139763	7999.968150	13.845338	-0.090820	4.817977
463.509614	8000.312341	13.850343	-0.090889	4.818077
463.623916	8000.285524	13.855347	-0.090910	4.818069
463.435439	8000.177597	13.860352	-0.090875	4.818038
463.600117	8000.218865	13.865357	-0.090906	4.818049
463.291818	8000.033457	13.870362	-0.090848	4.817995
463.117838	8000.049963	13.875367	-0.090816	4.818001
463.381967	8000.150530	13.880371	-0.090865	4.818030
463.444032	8000.062970	13.885376	-0.090877	4.818004
462.858215	8000.109484	13.890381	-0.090768	4.818020
463.255304	7999.991891	13.895386	-0.090841	4.817983
463.215126	8000.103973	13.900391	-0.090834	4.818017
463.545947	8000.311810	13.905395	-0.090896	4.818077
463.200045	8000.211146	13.910400	-0.090831	4.818049
463.048676	8000.130062	13.915405	-0.090803	4.818025
462.816638	7999.967837	13.920410	-0.090760	4.817978
462.991537	8000.217693	13.925415	-0.090793	4.818051
462.427023	7999.821301	13.930419	-0.090687	4.817936
463.234177	8000.165308	13.935424	-0.090838	4.818035
463.373332	8000.133576	13.940429	-0.090864	4.818025
463.416403	8000.098388	13.945434	-0.090872	4.818014
463.215716	8000.350340	13.950439	-0.090834	4.818090
463.105159	8000.016112	13.955443	-0.090814	4.817991
463.408549	8000.306731	13.960448	-0.090870	4.818076
463.662349	8000.139748	13.965453	-0.090917	4.818025
463.686752	8000.153779	13.970458	-0.090922	4.818029
463.548170	8000.326594	13.975463	-0.090896	4.818081
463.731822	8000.156520	13.980467	-0.090930	4.818030
463.825858	8000.335764	13.985472	-0.090948	4.818083
463.722979	8000.247989	13.990477	-0.090929	4.818057
463.880020	8000.105966	13.995482	-0.090958	4.818014
463.323970	8000.225538	14.000487	-0.090855	4.818052
463.097323	8000.169715	14.005491	-0.090812	4.818037
463.521360	8000.152515	14.010496	-0.090891	4.818030
463.634288	8000.338340	14.015501	-0.090913	4.818084
463.355142	8000.012268	14.020506	-0.090860	4.817989
463.309632	8000.345358	14.025511	-0.090852	4.818088
463.714069	7999.984677	14.030515	-0.090927	4.817979
463.464751	8000.268582	14.035520	-0.090881	4.818064
463.021828	8000.072860	14.040525	-0.090798	4.818008
463.328675	8000.004532	14.045530	-0.090855	4.817987
463.266259	8000.182626	14.050535	-0.090844	4.818040
463.094184	7999.909650	14.055539	-0.090812	4.817960
463.078368	8000.082080	14.060544	-0.090809	4.818011
462.898126	8000.076391	14.065549	-0.090775	4.818010
463.021913	7999.959169	14.070554	-0.090798	4.817975
462.949096	8000.115008	14.075559	-0.090785	4.818021
463.424516	8000.162748	14.080563	-0.090874	4.818033
463.421998	8000.278519	14.085568	-0.090873	4.818068
463.173103	8000.246596	14.090573	-0.090827	4.818059
462.718077	7999.826473	14.095578	-0.090742	4.817936
462.892451	8000.001572	14.100583	-0.090774	4.817988
462.547929	7999.940939	14.105587	-0.090710	4.817971
462.452789	7999.917497	14.110592	-0.090693	4.817965
462.520952	7999.854238	14.115597	-0.090705	4.817945
462.701025	7999.808342	14.120602	-0.090739	4.817931
462.930354	8000.061064	14.125607	-0.090782	4.818005
463.619183	8000.319200	14.130611	-0.090910	4.818079
463.400312	8000.167682	14.135616	-0.090869	4.818035
462.780410	7999.847359	14.140621	-0.090754	4.817942
463.064662	7999.932413	14.145626	-0.090807	4.817966
463.163060	8000.227517	14.150631	-0.090825	4.818054
463.182054	8000.005651	14.155635	-0.090828	4.817988
462.725594	7999.920285	14.160640	-0.090743	4.817964
463.116967	8000.043691	14.165645	-0.090816	4.817999
463.211712	7999.975541	14.170650	-0.090834	4.817979
463.175314	8000.040302	14.175655	-0.090827	4.817998
463.212268	8000.031347	14.180659	-0.090834	4.817995
462.990487	7999.992439	14.185664	-0.090793	4.817985
462.918173	7999.914573	14.190669	-0.090779	4.817962
463.512293	8000.195587	14.195674	-0.090890	4.818043
463.301575	8000.214735	14.200679	-0.090851	4.818049
463.053871	7999.917535	14.205683	-0.090805	4.817962
462.408973	7999.852684	14.210688	-0.090685	4.817945
462.272582	7999.728655	14.215693	-0.090659	4.817909
462.416662	7999.846478	14.220698	-0.090686	4.817944
462.396168	7999.933568	14.225703	-0.090682	4.817970
461.990193	7999.780488	14.230707	-0.090607	4.817926
461.905873	7999.899315	14.235712	-0.090591	4.817961
462.183690	7999.831631	14.240717	-0.090643	4.817940
462.451152	7999.773276	14.245722	-0.090692	4.817922
462.127025	7999.828732	14.250727	-0.090632	4.817940
462.202161	7999.854001	14.255731	-0.090646	4.817947
462.477189	7999.834703	14.260736	-0.090697	4.817940
462.535354	7999.738669	14.265741	-0.090708	4.817911
462.766284	7999.848238	14.270746	-0.090751	4.817943
462.643302	7999.920204	14.275751	-0.090728	4.817965
462.927785	7999.924200	14.280755	-0.090781	4.817965
462.548621	7999.910455	14.285760	-0.090711	4.817962
462.512813	7999.866791	14.290765	-0.090704	4.817949
462.936335	7999.816944	14.295770	-0.090783	4.817933
462.704749	7999.914756	14.300775	-0.090740	4.817963
462.971232	7999.956398	14.305779	-0.090790	4.817974
462.516614	7999.539451	14.310784	-0.090705	4.817852

462.805336	7996.430911	14.315789	-0.090756	4.816929
462.790488	7990.802822	14.320794	-0.090750	4.815259
462.604441	7984.057399	14.325799	-0.090711	4.813258
462.223458	7976.868591	14.330803	-0.090635	4.811125
462.552812	7969.082075	14.335808	-0.090692	4.808811
462.776185	7961.320911	14.340813	-0.090728	4.806503
462.272002	7953.402841	14.345818	-0.090629	4.804151
461.963274	7945.600452	14.350823	-0.090567	4.801831
462.525806	7937.510856	14.355827	-0.090666	4.799421
462.499223	7929.591844	14.360832	-0.090656	4.797063
462.317952	7921.496768	14.365837	-0.090617	4.794652
462.282732	7913.634808	14.370842	-0.090605	4.792309
462.205724	7905.541789	14.375847	-0.090586	4.789895
462.297115	7897.509229	14.380851	-0.090597	4.787498
461.924949	7889.538129	14.385856	-0.090523	4.785120
461.840562	7881.561817	14.390861	-0.090502	4.782738
462.205260	7873.512980	14.395866	-0.090565	4.780331
462.058824	7865.525191	14.400871	-0.090532	4.777944
462.338923	7857.544933	14.405875	-0.090579	4.775556
461.822057	7849.552982	14.410880	-0.090478	4.773165
461.494912	7841.563008	14.415885	-0.090412	4.770774
461.666482	7833.557160	14.420890	-0.090438	4.768375
461.613453	7825.484352	14.425895	-0.090423	4.765955
461.161110	7817.560667	14.430899	-0.090334	4.763580
461.625829	7809.528043	14.435904	-0.090415	4.761169
461.963658	7801.416009	14.440909	-0.090473	4.758733
461.599652	7793.613433	14.445914	-0.090400	4.756391
461.395247	7785.510881	14.450919	-0.090357	4.753956
462.015987	7777.452921	14.455923	-0.090467	4.751532
461.652860	7769.459012	14.460928	-0.090394	4.749128
460.918639	7761.560611	14.465933	-0.090252	4.746753
461.296958	7753.452560	14.470938	-0.090318	4.744311
461.380575	7745.470553	14.475943	-0.090328	4.741906
461.643123	7737.459773	14.480947	-0.090372	4.739491
461.070266	7729.566793	14.485952	-0.090260	4.737112
461.702255	7721.378516	14.490957	-0.090372	4.734640
461.493921	7713.470583	14.495962	-0.090328	4.732253
461.510712	7705.479408	14.500967	-0.090326	4.729839
461.832469	7697.438584	14.505971	-0.090381	4.727409
461.433037	7689.428053	14.510976	-0.090301	4.724988
460.581333	7681.562357	14.515981	-0.090138	4.722610
460.673748	7673.552044	14.520986	-0.090150	4.720186
460.509782	7665.527809	14.525991	-0.090114	4.717756
460.637162	7657.512540	14.530995	-0.090132	4.715327
460.567748	7649.495122	14.536000	-0.090114	4.712897
460.483826	7641.491059	14.541005	-0.090093	4.710470
461.081921	7633.420616	14.546010	-0.090200	4.708020
460.968093	7625.368100	14.551015	-0.090173	4.705576
460.782216	7617.451003	14.556019	-0.090133	4.703171
461.163980	7609.421495	14.561024	-0.090199	4.700730
460.967005	7601.441731	14.566029	-0.090157	4.698304
461.063995	7593.471507	14.571034	-0.090170	4.695879
460.765452	7585.453547	14.576039	-0.090109	4.693439
460.934360	7577.489824	14.581043	-0.090136	4.691014
460.409500	7569.476449	14.586048	-0.090033	4.688573
460.820603	7561.432764	14.591053	-0.090104	4.686120
460.733354	7553.450890	14.596058	-0.090083	4.683685
460.451335	7545.517621	14.601063	-0.090025	4.681265
460.852342	7537.439215	14.606067	-0.090094	4.678798
460.939563	7529.475460	14.611072	-0.090105	4.676365
460.697525	7521.436394	14.616077	-0.090055	4.673908
460.528478	7513.486531	14.621082	-0.090019	4.671476
460.383027	7505.397101	14.626087	-0.089986	4.669001
460.523348	7497.442033	14.631091	-0.090007	4.666566
459.905387	7489.411354	14.636096	-0.089887	4.664106
460.309035	7481.446740	14.641101	-0.089957	4.661665
459.873095	7473.447424	14.646106	-0.089870	4.659213
459.598577	7465.511677	14.651111	-0.089814	4.656778
459.907004	7457.416999	14.656115	-0.089866	4.654293
459.969301	7449.463562	14.661120	-0.089873	4.651851
459.450669	7441.452042	14.666125	-0.089771	4.649389
460.222064	7433.404748	14.671130	-0.089909	4.646915
459.954838	7425.376563	14.676135	-0.089854	4.644445
459.979633	7417.449075	14.681139	-0.089854	4.642005
460.090796	7409.426397	14.686144	-0.089869	4.639535
460.134281	7401.443447	14.691149	-0.089872	4.637075
459.944747	7393.448680	14.696154	-0.089832	4.634611
459.556764	7385.460444	14.701159	-0.089754	4.632147
459.771675	7377.332356	14.706163	-0.089789	4.629639
459.626026	7369.388986	14.711168	-0.089757	4.627186
459.167268	7361.337191	14.716173	-0.089666	4.624699
459.130729	7353.478048	14.721178	-0.089654	4.622269
458.852924	7345.403488	14.726183	-0.089597	4.619772
458.757995	7337.490394	14.731187	-0.089574	4.617323
458.475586	7329.413601	14.736192	-0.089517	4.614823
458.518640	7321.419107	14.741197	-0.089519	4.612346
458.620727	7313.414645	14.746202	-0.089533	4.609866
458.512742	7305.339563	14.751207	-0.089508	4.607361
458.803346	7297.306955	14.756211	-0.089557	4.604869
458.581345	7289.471263	14.761216	-0.089510	4.602437
458.496209	7281.365009	14.766221	-0.089489	4.599919
459.074111	7273.375350	14.771226	-0.089592	4.597437
459.123265	7265.344610	14.776231	-0.089596	4.594940
459.063684	7257.391895	14.781235	-0.089579	4.592465
458.749016	7249.355320	14.786240	-0.089515	4.589963
458.689501	7241.309116	14.791245	-0.089499	4.587457
458.553972	7233.348818	14.796250	-0.089469	4.584977
457.994720	7225.415926	14.801255	-0.089359	4.582502
457.963866	7217.354864	14.806259	-0.089348	4.579988
458.036022	7209.413714	14.811264	-0.089357	4.577509
457.634574	7201.350451	14.816269	-0.089277	4.574990
457.933911	7193.382807	14.821274	-0.089327	4.572501
458.008408	7185.266942	14.826279	-0.089336	4.569964
457.997691	7177.350629	14.831283	-0.089329	4.567487
457.725193	7169.316569	14.836288	-0.089273	4.564972
457.528357	7161.387237	14.841293	-0.089231	4.562489
457.911248	7153.335019	14.846298	-0.089297	4.559967
457.676063	7145.358952	14.851303	-0.089248	4.557466
457.982377	7137.284132	14.856307	-0.089300	4.554933
457.780155	7129.366462	14.861312	-0.089257	4.552448
457.342747	7121.352543	14.866317	-0.089170	4.549930
457.648801	7113.262187	14.871322	-0.089222	4.547389
457.675953	7105.230007	14.876327	-0.089222	4.544864
457.708464	7097.313378	14.881331	-0.089223	4.542374
457.054593	7089.377855	14.886336	-0.089096	4.539875
456.841289	7081.363050	14.891341	-0.089051	4.537350
457.382148	7073.283029	14.896346	-0.089147	4.534806
457.088106	7065.311576	14.901351	-0.089087	4.532292
456.613165	7057.332416	14.906355	-0.088993	4.529774
456.903604	7049.332187	14.911360	-0.089042	4.527250
456.823600	7041.286358	14.916365	-0.089022	4.524709
456.525371	7033.388402	14.921370	-0.088961	4.522212
456.420671	7025.302530	14.926375	-0.088936	4.519656
456.835033	7017.315850	14.931379	-0.089008	4.517131
456.672665	7009.269231	14.936384	-0.088973	4.514583
456.234043	7001.332544	14.941389	-0.088886	4.512069
456.203270	6993.338109	14.946394	-0.088875	4.509535
455.861184	6985.275677	14.951399	-0.088806	4.506978
455.740491	6977.238208	14.956403	-0.088778	4.504428
455.857255	6969.292224	14.961408	-0.088795	4.501906
455.571016	6961.247049	14.966413	-0.088736	4.499350
455.606483	6953.294258	14.971418	-0.088738	4.496823
455.939399	6945.103948	14.976423	-0.088795	4.494221
456.079808	6937.228589	14.981427	-0.088816	4.491716
456.006068	6929.174807	14.986432	-0.088797	4.489152
455.960708	6921.231159	14.991437	-0.088783	4.486622
456.107277	6913.197583	14.996442	-0.088805	4.484063
455.910066	6905.285423	15.001447	-0.088763	4.481539
455.866294	6897.217363	15.006451	-0.088750	4.478965
455.776214	6889.266030	15.011456	-0.088728	4.476426
456.316964	6881.127267	15.016461	-0.088823	4.473829
455.930336	6873.230966	15.021466	-0.088746	4.471304
455.850115	6865.157502	15.026471	-0.088726	4.468722
456.007494	6857.179141	15.031475	-0.088750	4.466170
456.174963	6849.162248	15.036480	-0.088776	4.463605
456.265998	6841.156829	15.041485	-0.088788	4.461041
456.532441	6833.171010	15.046490	-0.088832	4.458483
456.226770	6825.243696	15.051495	-0.088770	4.455939
456.209436	6817.167012	15.056499	-0.088762	4.453348
455.976296	6809.235323	15.061504	-0.088713	4.450800
456.071563	6801.158567	15.066509	-0.088726	4.448206
456.146203	6793.196534	15.071514	-0.088734	4.445647
456.185875	6785.180404	15.076519	-0.088736	4.443069
456.099566	6777.214533	15.081523	-0.088715	4.440506
456.087158	6769.212393	15.086528	-0.088708	4.437929
456.400162	6761.097323	15.091533	-0.088761	4.435316
456.320746	6753.183049	15.096538	-0.088741	4.432765
455.989965	6745.199114	15.101543	-0.088674	4.430188
455.605664	6737.221820	15.106547	-0.088597	4.427611
455.725874	6729.174170	15.111552	-0.088614	4.425013
455.537843	6721.169284	15.116557	-0.088574	4.422426
455.770188	6713.134913	15.121562	-0.088612	4.419829
455.659981	6705.185420	15.126567	-0.088587	4.417257
456.016541	6697.126343	15.131571	-0.088648	4.414650
455.289514	6689.238581	15.136576	-0.088507	4.412092
455.047297	6681.190963	15.141581	-0.088457	4.409482
455.459495	6673.208524	15.146586	-0.088528	4.406896
454.884079	6665.133299	15.151591	-0.088416	4.404273
454.785824	6657.227324	15.156595	-0.088393	4.401706
455.015185	6649.192082	15.161600	-0.088430	4.399097
455.466280	6641.144843	15.166605	-0.088509	4.396484
455.742247	6633.132436	15.171610	-0.088555	4.393880
455.769004	6625.138122	15.176615	-0.088555	4.391279
455.521842	6617.126088	15.181619	-0.088504	4.388669
455.832877	6609.139544	15.186624	-0.088556	4.386069
455.542776	6601.164792	15.191629	-0.088497	4.383467
455.656133	6593.204016	15.196634	-0.088513	4.380871
455.546673	6585.220884	15.201639	-0.088487	4.378265
454.683488	6577.297174	15.206643	-0.088322	4.375671
454.431909	6569.244574	15.211648	-0.088270	4.373038
454.641452	6561.213081	15.216653	-0.088303	4.370414
454.510336	6553.279370	15.221658	-0.088274	4.367817
454.133593	6545.238391	15.226663	-0.088198	4.365182
454.203282	6537.298611	15.231667	-0.088206	4.362582
454.170867	6529.234347	15.236672	-0.088195	4.359938
453.804829	6521.293624	15.241677	-0.088122	4.357331
453.894678	6513.267873	15.246682	-0.088133	4.354698
454.374421	6505.164141	15.251687	-0.088217	4.352041
454.317256	6497.135159	15.256691	-0.088201	4.349402
454.001614	6489.167241	15.261696	-0.088137	4.346781
454.602592	6481.051476	15.266701	-0.088244	4.344115
454.487621	6473.235700	15.271706	-0.088217	4.341542
454.118909	6465.175583	15.276711	-0.088144	4.338884
454.109039	6457.257064	15.281715	-0.088137	4.336275
454.250677	6449.210085	15.286720	-0.088158	4.333622
454.093951	6441.228048	15.291725	-0.088123	4.330987
454.174998	6433.216880	15.296730	-0.088133	4.328343
454.556508	6425.140024	15.301735	-0.088199	4.325678
454.396559	6417.240754	15.306739	-0.088164	4.323065
454.490601	6409.199500	15.311744	-0.088176	4.320406
454.440248	6401.245008	15.316749	-0.088162	4.317773
454.231772	6393.272953	15.321754	-0.088118	4.315131
454.262931	6385.218850	15.326759	-0.088118	4.312463
453.795210	6377.242605	15.331763	-0.088026	4.309814
453.938875	6369.230457	15.336768	-0.088048	4.307157
453.945750	6361.138353	15.341773	-0.088044	4.304470
453.715910	6353.266949	15.346778	-0.087996	4.301853
453.760486	6345.151967	15.351783	-0.087999	4.299156
453.646174	6337.207639	15.356787	-0.087972	4.296513
453.628059	6329.114728	15.361792	-0.087964	4.293819
453.921655	6321.110432	15.366797	-0.088013	4.291156
454.295694	6313.117262	15.371802	-0.088078	4.288496
453.770560	6305.182270	15.376807	-0.087975	4.285845
453.533057	6297.194986	15.381811	-0.087925	4.283178
453.412444	6289.239486	15.386816	-0.087898	4.280521
453.802616	6281.173021	15.391821	-0.087965	4.277830
453.309405	6273.249059	15.396826	-0.087868	4.275177
453.072973	6265.225050	15.401831	-0.087819	4.272490
453.131018	6257.183887	15.406835	-0.087824	4.269800
453.018108	6249.138661	15.411840	-0.087798	4.267104
452.553360	6241.196188	15.416845	-0.087706	4.264438
453.282667	6233.152794	15.421850	-0.087837	4.261748
452.832755	6225.148410	15.426855	-0.087748	4.259057
452.612214	6217.225303	15.431859	-0.087702	4.256395
452.883913	6209.159935	15.436864	-0.087747	4.253688
452.586679	6201.172141	15.441869	-0.087687	4.250999
452.321831	6193.182998	15.446874	-0.087632	4.248309
452.006698	6185.174579	15.451879	-0.087568	4.245610
452.420876	6177.135474	15.456883	-0.087640	4.242907
452.646953	6169.125567	15.461888	-0.087677	4.240209
452.378307	6161.173739	15.466893	-0.087622	4.237525
452.505714	6153.180664	15.471898	-0.087640	4.234828
452.111840	6145.183821	15.476903	-0.087562	4.232124
452.438331	6137.122711	15.481907	-0.087617	4.229403
452.948938	6129.093196	15.486912	-0.087707	4.226694
452.210587	6121.162448	15.491917	-0.087565	4.224003
452.263879	6113.236829	15.496922	-0.087569	4.221320
451.785670	6105.203308	15.501927	-0.087475	4.218593
451.571072	6097.213670	15.506931	-0.087430	4.215882
451.762049	6089.157275	15.511936	-0.087460	4.213151
451.741962	6081.103701	15.516941	-0.087451	4.210417
451.776049	6073.185917	15.521946	-0.087453	4.207728
451.488355	6065.152463	15.526951	-0.087394	4.204995
451.374964	6057.199344	15.531955	-0.087367	4.202289
451.520548	6049.162996	15.536960	-0.087389	4.199555
451.323998	6041.196439	15.541965	-0.087348	4.196840
451.255135	6033.171294	15.546970	-0.087329	4.194105
451.665287	6025.070210	15.551975	-0.087401	4.191347
451.473125	6017.062503	15.556979	-0.087360	4.188612
451.214506	6009.150139	15.561984	-0.087306	4.185908
451.237655	6001.109060	15.566989	-0.087305	4.183161
451.492043	5993.094462	15.571994	-0.087348	4.180424
451.603175	5985.095480	15.576999	-0.087363	4.177689
451.437141	5977.123262	15.582003	-0.087327	4.174957
451.555170	5969.129930	15.587008	-0.087344	4.172221
451.392311	5961.088928	15.592013	-0.087308	4.169462
451.018961	5953.186382	15.597018	-0.087234	4.166747
450.871113	5945.122858	15.602023	-0.087201	4.163978
451.099928	5937.183871	15.607027	-0.087238	4.161254
450.504021	5929.244435	15.612032	-0.087122	4.158518
450.213439	5921.227676	15.617037	-0.087063	4.155757
450.272682	5913.233497	15.622042	-0.087069	4.153006
450.395829	5905.155247	15.627047	-0.087086	4.150226
450.110665	5897.207049	15.632051	-0.087028	4.147483
450.125265	5889.153536	15.637056	-0.087025	4.144706
450.343193	5881.151186	15.642061	-0.087061	4.141948
450.014484	5873.159252	15.647066	-0.086994	4.139184
449.902459	5865.205263	15.652071	-0.086968	4.136434
450.516501	5857.084644	15.657075	-0.087077	4.133634
450.152577	5849.198711	15.662080	-0.087005	4.130901
449.888104	5841.177329	15.667085	-0.086950	4.128120
449.728924	5833.252895	15.672090	-0.086915	4.125372
449.911934	5825.226942	15.677095	-0.086944	4.122592
449.679735	5817.206303	15.682099	-0.086896	4.119806
449.760873	5809.213996	15.687104	-0.086906	4.117033
449.574898	5801.175562	15.692109	-0.086866	4.114238
449.559034	5793.232912	15.697114	-0.086858	4.111476
449.313415	5785.154014	15.702119	-0.086807	4.108662
449.492576	5777.120295	15.707123	-0.086835	4.105868
449.432815	5769.174124	15.712128	-0.086819	4.103099
449.287325	5761.170549	15.717133	-0.086786	4.100307
449.996575	5753.154006	15.722138	-0.086913	4.097521
450.096538	5745.097666	15.727143	-0.086926	4.094710
450.035991	5737.151665	15.732147	-0.086910	4.091934
449.607121	5729.183351	15.737152	-0.086825	4.089142
449.798831	5721.187038	15.742157	-0.086856	4.086348
449.345175	5713.219298	15.747162	-0.086766	4.083553
449.308513	5705.215792	15.752167	-0.086754	4.080749
449.608251	5697.133396	15.757171	-0.086804	4.077920
449.704882	5689.145996	15.762176	-0.086817	4.075120
449.585906	5681.142034	15.767181	-0.086790	4.072309
449.723100	5673.137234	15.772186	-0.086810	4.069500
450.102606	5665.108942	15.777191	-0.086876	4.066684
449.770245	5657.157343	15.782195	-0.086809	4.063882
449.888657	5649.204409	15.787200	-0.086825	4.061085
450.138194	5641.123650	15.792205	-0.086867	4.058242
449.786137	5633.215343	15.797210	-0.086796	4.055450
449.661048	5625.206296	15.802215	-0.086767	4.052623
449.477089	5617.205474	15.807219	-0.086728	4.049796
449.335950	5609.231413	15.812224	-0.086697	4.046978
449.159625	5601.145322	15.817229	-0.086658	4.044117
449.222836	5593.275007	15.822234	-0.086665	4.041334
448.898215	5585.222796	15.827239	-0.086599	4.038479
449.283397	5577.174627	15.832243	-0.086666	4.035635
449.132717	5569.186873	15.837248	-0.086633	4.032801
449.301014	5561.083062	15.842253	-0.086659	4.029930
449.006554	5553.186187	15.847258	-0.086599	4.027122
448.676995	5545.167384	15.852263	-0.086532	4.024269
448.358484	5537.270687	15.857267	-0.086468	4.021457
448.700184	5529.205454	15.862272	-0.086526	4.018593
448.784124	5521.161221	15.867277	-0.086537	4.015732
448.529278	5513.233878	15.872282	-0.086484	4.012904
448.510179	5505.167322	15.877287	-0.086475	4.010028
448.530120	5497.204484	15.882291	-0.086474	4.007188
448.056956	5489.241551	15.887296	-0.086380	4.004337
447.676161	5481.325578	15.892301	-0.086304	4.001503
448.155361	5473.227194	15.897306	-0.086388	3.998616
448.306451	5465.189292	15.902311	-0.086411	3.995744
448.427856	5457.204732	15.907315	-0.086429	3.992887
448.336597	5449.230789	15.912320	-0.086406	3.990029
448.076858	5441.219337	15.917325	-0.086353	3.987152
447.670494	5433.273049	15.922330	-0.086272	3.984295
447.652106	5425.287775	15.927335	-0.086263	3.981427
447.638712	5417.253303	15.932339	-0.086256	3.978540
447.803495	5409.225525	15.937344	-0.086281	3.975657
447.810515	5401.196495	15.942349	-0.086277	3.972768
448.063607	5393.162936	15.947354	-0.086319	3.969880
448.167853	5385.200505	15.952359	-0.086333	3.967013
447.962941	5377.182960	15.957363	-0.086290	3.964118
447.736465	5369.323788	15.962368	-0.086243	3.961278
447.900837	5361.203655	15.967373	-0.086268	3.958349
447.947928	5353.253389	15.972378	-0.086272	3.955476
448.181939	5345.207134	15.977383	-0.086310	3.952571
448.033890	5337.216201	15.982387	-0.086277	3.949676
448.100824	5329.240104	15.987392	-0.086285	3.946788
448.216216	5321.132168	15.992397	-0.086301	3.943852
448.101793	5313.279457	15.997402	-0.086274	3.941001
448.017437	5305.249521	16.002407	-0.086253	3.938085
447.873750	5297.269873	16.007411	-0.086221	3.935184
447.975777	5289.282612	16.012416	-0.086235	3.932282
447.772668	5281.214104	16.017421	-0.086192	3.929343
447.621121	5273.279339	16.022426	-0.086159	3.926452
447.670244	5265.272324	16.027431	-0.086163	3.923535
447.632750	5257.281788	16.032435	-0.086151	3.920621
447.597268	5249.270593	16.037440	-0.086139	3.917698
447.376765	5241.261511	16.042445	-0.086093	3.914769
447.324427	5233.320483	16.047450	-0.086078	3.911866
447.290773	5225.295629	16.052455	-0.086066	3.908931
446.929472	5217.319072	16.057459	-0.085994	3.906004
447.421087	5209.236424	16.062464	-0.086080	3.903054
447.592039	5201.212714	16.067469	-0.086107	3.900116
447.042510	5193.346229	16.072474	-0.085999	3.897220
447.229903	5185.265625	16.077479	-0.086029	3.894258
447.231174	5177.322711	16.082483	-0.086024	3.891340
447.113625	5169.285289	16.087488	-0.085997	3.888383
446.641189	5161.338810	16.092493	-0.085904	3.885449
447.467551	5153.290642	16.097498	-0.086052	3.882503
447.263578	5145.274626	16.102503	-0.086009	3.879545
446.883932	5137.374416	16.107507	-0.085933	3.876624
446.851736	5129.322323	16.112512	-0.085922	3.873652
446.818775	5121.189437	16.117517	-0.085911	3.870648
446.657047	5113.259232	16.122522	-0.085875	3.867713
446.442387	5105.287472	16.127527	-0.085830	3.864760
446.494259	5097.303506	16.132531	-0.085835	3.861806
446.624031	5089.308592	16.137536	-0.085854	3.858847
446.536151	5081.297601	16.142541	-0.085832	3.855875
446.207893	5073.356148	16.147546	-0.085766	3.852922
446.229050	5065.315236	16.152551	-0.085764	3.849936
445.818546	5057.369137	16.157555	-0.085683	3.846975
446.445409	5049.283220	16.162560	-0.085794	3.843981
445.910356	5041.397869	16.167565	-0.085690	3.841035
445.978133	5033.345640	16.172570	-0.085697	3.838037
445.455285	5025.416051	16.177575	-0.085594	3.835070
445.897516	5017.341189	16.182579	-0.085672	3.832067
445.962543	5009.326303	16.187584	-0.085678	3.829076
445.681959	5001.312053	16.192589	-0.085621	3.826076
445.845788	4993.317270	16.197594	-0.085646	3.823090
445.702153	4985.352674	16.202599	-0.085614	3.820106
445.571673	4977.401922	16.207603	-0.085585	3.817126
445.477170	4969.352058	16.212608	-0.085562	3.814106
445.393123	4961.368725	16.217613	-0.085541	3.811110
445.457932	4953.341237	16.222618	-0.085548	3.808098
445.236675	4945.367994	16.227623	-0.085502	3.805097
445.402723	4937.382786	16.232627	-0.085527	3.802099
445.839383	4929.327744	16.237632	-0.085603	3.799077
445.576113	4921.396777	16.242637	-0.085549	3.796085
445.122091	4913.473853	16.247642	-0.085460	3.793088
444.824794	4905.474195	16.252647	-0.085399	3.790064
444.697237	4897.421892	16.257651	-0.085370	3.787021
444.687725	4889.401088	16.262656	-0.085363	3.783991
445.078286	4881.357945	16.267661	-0.085431	3.780958
445.087020	4873.378501	16.272666	-0.085427	3.777939
444.875275	4865.382025	16.277671	-0.085382	3.774906
445.232561	4857.355041	16.282675	-0.085444	3.771872
444.895919	4849.413855	16.287680	-0.085376	3.768852
445.014422	4841.375077	16.292685	-0.085393	3.765803
444.953862	4833.447642	16.297690	-0.085376	3.762789
444.835210	4825.426016	16.302695	-0.085349	3.759736
445.339202	4817.400341	16.307699	-0.085438	3.756694
445.231748	4809.442631	16.312704	-0.085412	3.753661
445.064184	4801.413353	16.317709	-0.085376	3.750596
444.875558	4793.488591	16.322714	-0.085336	3.747569
445.068855	4785.397958	16.327719	-0.085366	3.744484
444.801399	4777.495367	16.332723	-0.085312	3.741458
444.426749	4769.544984	16.337728	-0.085237	3.738409
444.332229	4761.544864	16.342733	-0.085214	3.735344
444.251728	4753.551264	16.347738	-0.085194	3.732281
444.194280	4745.423575	16.352743	-0.085178	3.729163
444.058976	4737.503799	16.357747	-0.085147	3.726121
444.391657	4729.440536	16.362752	-0.085204	3.723033
444.895331	4721.415663	16.367757	-0.085293	3.719962
444.589711	4713.548526	16.372762	-0.085231	3.716928
444.002582	4705.556519	16.377767	-0.085116	3.713837
444.226528	4697.436850	16.382771	-0.085152	3.710714
444.232581	4689.459757	16.387776	-0.085148	3.707638
443.621927	4681.497116	16.392781	-0.085029	3.704550
443.361392	4673.593198	16.397786	-0.084976	3.701490
443.764165	4665.489334	16.402791	-0.085046	3.698368
444.066853	4657.447246	16.407795	-0.085097	3.695264
444.253528	4649.467136	16.412800	-0.085126	3.692179
443.489163	4641.528752	16.417805	-0.084979	3.689083
443.409151	4633.605011	16.422810	-0.084959	3.686007
443.467585	4625.542678	16.427815	-0.084964	3.682879
443.252388	4617.559598	16.432819	-0.084919	3.679772
443.454684	4609.592610	16.437824	-0.084952	3.676679
443.348858	4601.529027	16.442829	-0.084927	3.673538
443.743021	4593.519821	16.447834	-0.084995	3.670429
443.328125	4585.571277	16.452839	-0.084912	3.667319
443.402073	4577.522367	16.457843	-0.084921	3.664180
443.201728	4569.622363	16.462848	-0.084879	3.661090
443.300017	4561.565490	16.467853	-0.084892	3.657943
443.023096	4553.657283	16.472858	-0.084835	3.654842
442.975141	4545.586910	16.477863	-0.084821	3.651681
443.448057	4537.517383	16.482867	-0.084904	3.648532
443.561140	4529.545101	16.487872	-0.084919	3.645409
443.648348	4521.570298	16.492877	-0.084930	3.642281
443.471571	4513.643170	16.497882	-0.084892	3.639161
443.289691	4505.692331	16.502887	-0.084853	3.636030
443.006138	4497.673172	16.507891	-0.084795	3.632866
443.261508	4489.632319	16.512896	-0.084838	3.629706
443.054592	4481.618655	16.517901	-0.084794	3.626541
442.704215	4473.694312	16.522906	-0.084724	3.623404
442.155392	4465.701139	16.527911	-0.084616	3.620232
442.456321	4457.682566	16.532915	-0.084667	3.617071
443.034120	4449.572827	16.537920	-0.084769	3.613879
442.960651	4441.606119	16.542925	-0.084750	3.610723
443.159452	4433.604640	16.547930	-0.084782	3.607557
443.032917	4425.634524	16.552935	-0.084753	3.604392
442.909833	4417.681438	16.557939	-0.084725	3.601231
442.794446	4409.730122	16.562944	-0.084699	3.598068
442.829231	4401.702670	16.567949	-0.084700	3.594877
442.558988	4393.772938	16.572954	-0.084645	3.591712
442.080661	4385.788101	16.577959	-0.084550	3.588517
441.859474	4377.750143	16.582963	-0.084504	3.585305
442.039327	4369.757832	16.587968	-0.084532	3.582120
441.872818	4361.696707	16.592973	-0.084496	3.578895
442.529119	4353.658195	16.597978	-0.084613	3.575700
442.616471	4345.657320	16.602983	-0.084624	3.572500
442.348195	4337.674592	16.607987	-0.084569	3.569295
442.014455	4329.787354	16.612992	-0.084502	3.566123
442.453603	4321.695219	16.617997	-0.084578	3.562888
442.647209	4313.725858	16.623002	-0.084609	3.559693
442.551533	4305.771456	16.628007	-0.084586	3.556493
442.520218	4297.737180	16.633011	-0.084575	3.553259
442.361240	4289.740080	16.638016	-0.084540	3.550033
442.159000	4281.767554	16.643021	-0.084497	3.546813
441.674523	4273.833192	16.648026	-0.084402	3.543597
441.965453	4265.797465	16.653031	-0.084451	3.540361
442.124539	4257.780618	16.658035	-0.084475	3.537125
441.662789	4249.834989	16.663040	-0.084384	3.533896
441.222732	4241.874360	16.668045	-0.084297	3.530658
441.807026	4233.795091	16.673050	-0.084401	3.527402
441.417465	4225.808492	16.678055	-0.084323	3.524149
441.339893	4217.891277	16.683059	-0.084303	3.520932
441.592690	4209.851963	16.688064	-0.084345	3.517672
441.529254	4201.803263	16.693069	-0.084328	3.514396
441.435575	4193.877118	16.698074	-0.084305	3.511165
441.588479	4185.830252	16.703079	-0.084329	3.507890
441.289998	4177.884472	16.708083	-0.084268	3.504639
441.083921	4169.960319	16.713088	-0.084224	3.501396
441.310685	4161.858990	16.718093	-0.084261	3.498092
441.481258	4153.853568	16.723098	-0.084288	3.494823
441.248745	4145.907397	16.728103	-0.084239	3.491561
440.613397	4137.964298	16.733107	-0.084116	3.488284
440.642739	4129.965254	16.738112	-0.084116	3.485004
441.062696	4121.906766	16.743117	-0.084189	3.481708
441.091561	4113.924286	16.748122	-0.084189	3.478428
441.054543	4105.917461	16.753127	-0.084177	3.475132
441.164712	4097.909422	16.758131	-0.084193	3.471838
441.592196	4089.856050	16.763136	-0.084267	3.468532
440.532465	4081.994130	16.768141	-0.084065	3.465253
440.383257	4074.064722	16.773146	-0.084032	3.461973
440.012665	4066.077888	16.778151	-0.083957	3.458659
439.746211	4058.083606	16.783155	-0.083903	3.455341
439.884736	4050.027856	16.788160	-0.083923	3.452009
440.247599	4041.934344	16.793165	-0.083985	3.448666
440.900093	4033.890892	16.798170	-0.084102	3.445350
440.683486	4025.951236	16.803175	-0.084056	3.442044
440.843526	4017.976220	16.808179	-0.084081	3.438734
440.832826	4010.025188	16.813184	-0.084074	3.435424
440.456290	4002.059731	16.818189	-0.083998	3.432093
440.019506	3994.152095	16.823194	-0.083912	3.428780
439.648088	3986.146692	16.828199	-0.083838	3.425425
439.745650	3978.102680	16.833203	-0.083850	3.422068
440.267693	3970.039202	16.838208	-0.083942	3.418713
440.057609	3962.077611	16.843213	-0.083898	3.415373
439.977056	3954.113766	16.848218	-0.083878	3.412033
439.493481	3946.131473	16.853223	-0.083783	3.408667
440.069216	3938.072272	16.858227	-0.083885	3.405304
439.739631	3930.165720	16.863232	-0.083818	3.401969
440.335971	3922.057971	16.868237	-0.083924	3.398579
440.424137	3914.108694	16.873242	-0.083935	3.395234
440.290241	3906.101016	16.878247	-0.083905	3.391854
439.955752	3898.143670	16.883251	-0.083838	3.388484
439.916982	3890.128449	16.888256	-0.083825	3.385097
439.898721	3882.151985	16.893261	-0.083817	3.381723
440.132664	3874.155163	16.898266	-0.083855	3.378347
439.439785	3866.241713	16.903271	-0.083721	3.374969
439.267576	3858.237083	16.908275	-0.083684	3.371568
439.293036	3850.224232	16.913280	-0.083683	3.368167
439.000009	3842.202319	16.918285	-0.083623	3.364747
439.124619	3834.274875	16.923290	-0.083641	3.361380
438.523533	3826.348241	16.928295	-0.083524	3.357982
438.768362	3818.265232	16.933299	-0.083565	3.354546
438.668540	3810.282735	16.938304	-0.083541	3.351136
438.869744	3802.223551	16.943309	-0.083573	3.347701
439.200195	3794.213724	16.948314	-0.083629	3.344289
438.722492	3786.334922	16.953319	-0.083535	3.340898
438.326229	3778.377040	16.958323	-0.083456	3.337474
438.157416	3770.375369	16.963328	-0.083420	3.334036
437.887464	3762.392466	16.968333	-0.083364	3.330598
438.384953	3754.278538	16.973338	-0.083452	3.327130
438.654068	3746.247585	16.978343	-0.083496	3.323685
438.614522	3738.349491	16.983347	-0.083484	3.320282
438.176665	3730.448845	16.988352	-0.083397	3.316859
438.442313	3722.330779	16.993357	-0.083442	3.313366
438.390295	3714.373217	16.998362	-0.083427	3.309926
438.294210	3706.386077	17.003367	-0.083404	3.306468
438.510454	3698.340944	17.008371	-0.083439	3.302994
438.582938	3690.381264	17.013376	-0.083447	3.299547
438.226435	3682.455819	17.018381	-0.083375	3.296095
438.243883	3674.441647	17.023386	-0.083373	3.292615
438.589136	3666.364465	17.028391	-0.083432	3.289117
438.464209	3658.428956	17.033395	-0.083404	3.285658
438.642226	3650.437636	17.038400	-0.083432	3.282184
438.617643	3642.441066	17.043405	-0.083422	3.278695
438.829048	3634.461370	17.048410	-0.083456	3.275220
438.242132	3626.587781	17.053415	-0.083342	3.271755
437.807071	3618.606833	17.058419	-0.083256	3.268246
437.891563	3610.554604	17.063424	-0.083266	3.264722
438.076656	3602.525197	17.068429	-0.083296	3.261209
437.874776	3594.577232	17.073434	-0.083253	3.257712
437.976315	3586.557140	17.078439	-0.083266	3.254192
437.652442	3578.612986	17.083443	-0.083201	3.250684
437.603056	3570.614384	17.088448	-0.083187	3.247160
437.214705	3562.649134	17.093453	-0.083109	3.243632
437.021411	3554.710509	17.098458	-0.083068	3.240121
437.026339	3546.680747	17.103463	-0.083064	3.236573
437.124251	3538.656678	17.108467	-0.083077	3.233028
436.918272	3530.682017	17.113472	-0.083033	3.229488
437.247396	3522.579738	17.118477	-0.083089	3.225910
437.223870	3514.655401	17.123482	-0.083080	3.222393
436.511577	3506.749629	17.128487	-0.082942	3.218851
436.340987	3498.746662	17.133491	-0.082905	3.215284
436.665325	3490.701982	17.138496	-0.082960	3.211716
436.889476	3482.613354	17.143501	-0.082997	3.208120
436.857771	3474.675645	17.148506	-0.082985	3.204577
436.414695	3466.784088	17.153511	-0.082898	3.201032
436.555993	3458.729526	17.158515	-0.082919	3.197436
436.502381	3450.763355	17.163520	-0.082904	3.193867
436.687256	3442.713498	17.168525	-0.082933	3.190267
436.834252	3434.752788	17.173530	-0.082955	3.186701
436.225853	3426.826861	17.178535	-0.082837	3.183113
436.752938	3418.745158	17.183539	-0.082930	3.179502
436.585922	3410.806407	17.188544	-0.082893	3.175920
436.420740	3402.830143	17.193549	-0.082857	3.172317
436.626165	3394.815086	17.198554	-0.082890	3.168709
436.762061	3386.814480	17.203559	-0.082911	3.165100
436.659051	3378.859459	17.208563	-0.082886	3.161497
436.656327	3370.905088	17.213568	-0.082881	3.157895
436.336712	3362.949689	17.218573	-0.082816	3.154274
436.281065	3354.958309	17.223578	-0.082800	3.150645
436.702423	3346.866557	17.228583	-0.082873	3.146986
436.465905	3338.897139	17.233587	-0.082824	3.143350
436.550188	3330.934703	17.238592	-0.082835	3.139728
436.158720	3323.028697	17.243597	-0.082757	3.136105
436.171007	3315.014590	17.248602	-0.082754	3.132447
435.905610	3307.002728	17.253607	-0.082699	3.128773
436.011068	3299.000845	17.258611	-0.082714	3.125116
436.128339	3291.029570	17.263616	-0.082730	3.121469
436.173090	3283.006804	17.268621	-0.082733	3.117792
435.916755	3275.093060	17.273626	-0.082681	3.114146
435.484969	3267.149382	17.278631	-0.082595	3.110474
435.388309	3259.124542	17.283635	-0.082572	3.106775
435.995899	3251.028615	17.288640	-0.082680	3.103073
435.669031	3243.086762	17.293645	-0.082614	3.099393
435.509191	3235.193615	17.298650	-0.082579	3.095739
435.119073	3227.238840	17.303655	-0.082501	3.092042
435.268556	3219.143789	17.308659	-0.082523	3.088301
435.657101	3211.122905	17.313664	-0.082591	3.084600
435.141448	3203.240903	17.318669	-0.082489	3.080917
435.188905	3195.230991	17.323674	-0.082493	3.077197
435.299483	3187.203475	17.328679	-0.082508	3.073467
435.301621	3179.184748	17.333683	-0.082504	3.069732
435.143584	3171.240454	17.338688	-0.082469	3.066019
434.958794	3163.245156	17.343693	-0.082429	3.062276
435.160173	3155.270498	17.348698	-0.082462	3.058557
434.591025	3147.357966	17.353703	-0.082351	3.054826
434.492339	3139.350633	17.358707	-0.082327	3.051068
434.725198	3131.304103	17.363712	-0.082365	3.047303
435.023767	3123.256565	17.368717	-0.082416	3.043536
434.862413	3115.368994	17.373722	-0.082380	3.039817
434.296591	3107.487100	17.378727	-0.082270	3.036077
434.163184	3099.459414	17.383731	-0.082240	3.032284
434.275125	3091.446478	17.388736	-0.082255	3.028506
433.874286	3083.463767	17.393741	-0.082176	3.024712
434.242006	3075.464335	17.398746	-0.082239	3.020943
434.305809	3067.432399	17.403751	-0.082246	3.017140
434.270649	3059.441408	17.408755	-0.082234	3.013345
434.054241	3051.482333	17.413760	-0.082188	3.009552
434.125655	3043.476621	17.418765	-0.082196	3.005747
434.178889	3035.515038	17.423770	-0.082201	3.001957
433.901585	3027.581691	17.428775	-0.082144	2.998159
434.101527	3019.546199	17.433779	-0.082176	2.994331
434.379057	3011.558904	17.438784	-0.082223	2.990526
433.371177	3003.703034	17.443789	-0.082030	2.986713
433.935743	2995.608939	17.448794	-0.082130	2.982861
434.063154	2987.584998	17.453799	-0.082148	2.979016
434.020786	2979.624687	17.458803	-0.082135	2.975187
433.711208	2971.698290	17.463808	-0.082073	2.971356
433.034115	2963.765679	17.468813	-0.081941	2.967498
433.645699	2955.688687	17.473818	-0.082050	2.963632
433.776325	2947.674082	17.478823	-0.082069	2.959767
433.688516	2939.747786	17.483827	-0.082048	2.955927
433.877045	2931.747012	17.488832	-0.082078	2.952061
433.286053	2923.817829	17.493837	-0.081962	2.948184
433.567166	2915.764936	17.498842	-0.082009	2.944287
433.566457	2907.833583	17.503847	-0.082004	2.940429
433.427289	2899.827880	17.508851	-0.081973	2.936523
433.421868	2891.887951	17.513856	-0.081967	2.932651
433.366815	2883.839381	17.518861	-0.081951	2.928718
433.468519	2875.884553	17.523866	-0.081965	2.924834
433.391911	2867.908947	17.528871	-0.081946	2.920925
433.289474	2859.977462	17.533875	-0.081921	2.917031
433.210201	2851.992411	17.538880	-0.081902	2.913106
433.015701	2843.934485	17.543885	-0.081860	2.909135
433.298404	2835.913836	17.548890	-0.081907	2.905202
432.925419	2828.011734	17.553895	-0.081833	2.901286
433.576694	2819.934803	17.558899	-0.081949	2.897335
433.312988	2812.001094	17.563904	-0.081895	2.893399
433.048147	2804.047562	17.568909	-0.081840	2.889448
433.038174	2796.075841	17.573914	-0.081833	2.885497
432.926194	2788.108903	17.578919	-0.081807	2.881536
432.615125	2780.196726	17.583923	-0.081744	2.877587
432.799511	2772.182056	17.588928	-0.081773	2.873608
432.274479	2764.225313	17.593933	-0.081670	2.869613
432.769596	2756.152667	17.598938	-0.081757	2.865613
432.645789	2748.234192	17.603943	-0.081729	2.861648
432.640880	2740.252792	17.608947	-0.081723	2.857654
432.458042	2732.290955	17.613952	-0.081684	2.853653
432.217169	2724.308450	17.618957	-0.081634	2.849633
432.753310	2716.259253	17.623962	-0.081728	2.845619
432.655379	2708.312795	17.628967	-0.081705	2.841614
432.473514	2700.364914	17.633971	-0.081666	2.837598
432.045048	2692.475822	17.638976	-0.081581	2.833591
431.864618	2684.447419	17.643981	-0.081542	2.829523
432.284984	2676.384348	17.648986	-0.081615	2.825466
432.075046	2668.455729	17.653991	-0.081571	2.821435
432.194953	2660.419969	17.658995	-0.081588	2.817363
432.219076	2652.444884	17.664000	-0.081587	2.813310
431.795756	2644.515328	17.669005	-0.081503	2.809249
431.943126	2636.544728	17.674010	-0.081526	2.805194
431.449807	2628.636802	17.679015	-0.081429	2.801127
431.473598	2620.621868	17.684019	-0.081428	2.797030
431.809566	2612.599934	17.689024	-0.081485	2.792943
431.653400	2604.629995	17.694029	-0.081451	2.788846
431.665026	2596.632784	17.699034	-0.081448	2.784740
431.613838	2588.685051	17.704039	-0.081433	2.780649
431.647599	2580.703335	17.709043	-0.081434	2.776540
431.669011	2572.716724	17.714048	-0.081433	2.772421
431.374634	2564.743523	17.719053	-0.081373	2.768284
431.451615	2556.763931	17.724058	-0.081382	2.764161
431.425332	2548.811411	17.729063	-0.081372	2.760038
431.317255	2540.867238	17.734067	-0.081347	2.755909
431.486088	2532.819975	17.739072	-0.081373	2.751737
431.103113	2524.860516	17.744077	-0.081297	2.747571
431.080643	2516.874069	17.749082	-0.081287	2.743406
430.627465	2509.001849	17.754087	-0.081198	2.739268
430.592548	2501.001197	17.759091	-0.081186	2.735082
430.485146	2493.021471	17.764096	-0.081161	2.730896
430.932584	2484.910907	17.769101	-0.081239	2.726670
431.297624	2476.928837	17.774106	-0.081302	2.722500
431.217195	2469.004566	17.779111	-0.081281	2.718326
431.039477	2461.054478	17.784115	-0.081243	2.714126
431.103673	2453.104799	17.789120	-0.081250	2.709934
430.902965	2445.129106	17.794125	-0.081207	2.705706
430.953006	2437.151603	17.799130	-0.081212	2.701486
430.428284	2429.256100	17.804135	-0.081109	2.697266
430.616956	2421.236839	17.809139	-0.081139	2.693019
430.904506	2413.201101	17.814144	-0.081187	2.688764
430.947377	2405.206502	17.819149	-0.081190	2.684508
430.581577	2397.347411	17.824154	-0.081117	2.680290
430.581687	2389.369284	17.829159	-0.081111	2.676027
430.410077	2381.388136	17.834163	-0.081074	2.671743
430.234660	2373.431987	17.839168	-0.081036	2.667466
430.166041	2365.426812	17.844173	-0.081018	2.663163
429.726133	2357.543411	17.849178	-0.080931	2.658893
430.052093	2349.476843	17.854183	-0.080987	2.654569
429.956314	2341.491929	17.859187	-0.080964	2.650254
430.053228	2333.520832	17.864192	-0.080977	2.645952
429.725436	2325.588603	17.869197	-0.080910	2.641636
430.157568	2317.554787	17.874202	-0.080986	2.637308
430.046279	2309.629962	17.879207	-0.080960	2.632996
429.674109	2301.667424	17.884211	-0.080885	2.628639
429.897311	2293.640570	17.889216	-0.080922	2.624280
429.308755	2285.786562	17.894221	-0.080807	2.619952
429.539006	2277.774165	17.899226	-0.080845	2.615587
429.583052	2269.758107	17.904231	-0.080848	2.611200
429.779928	2261.752862	17.909235	-0.080879	2.606821
429.802323	2253.807496	17.914240	-0.080878	2.602457
429.684401	2245.861597	17.919245	-0.080851	2.598075
429.684631	2237.908948	17.924250	-0.080846	2.593690
429.520843	2229.833948	17.929255	-0.080810	2.589218
429.568998	2221.841553	17.934259	-0.080814	2.584799
429.705769	2213.897756	17.939264	-0.080834	2.580406
429.643124	2205.952441	17.944269	-0.080817	2.575991
429.301891	2198.050450	17.949274	-0.080749	2.571572
429.524857	2190.016217	17.954279	-0.080785	2.567112
429.180633	2182.115360	17.959283	-0.080716	2.562679
429.297649	2174.157150	17.964288	-0.080732	2.558238
428.605513	2166.278450	17.969293	-0.080598	2.553777
428.869398	2158.244966	17.974298	-0.080642	2.549289
428.995934	2150.238849	17.979303	-0.080661	2.544798
428.805355	2142.288197	17.984307	-0.080620	2.540309
428.772952	2134.340010	17.989312	-0.080609	2.535824
429.054378	2126.302398	17.994317	-0.080656	2.531303
428.712842	2118.404796	17.999322	-0.080587	2.526808
428.695600	2110.429084	18.004327	-0.080579	2.522285
428.686037	2102.474931	18.009331	-0.080572	2.517766
428.596059	2094.539412	18.014336	-0.080550	2.513244
428.075682	2086.615071	18.019341	-0.080448	2.508688
428.377730	2078.576250	18.024346	-0.080499	2.504119
428.107285	2070.659424	18.029351	-0.080443	2.499570
427.810115	2062.713303	18.034355	-0.080383	2.494993
428.091865	2054.680549	18.039360	-0.080430	2.490401
427.788161	2046.744946	18.044365	-0.080368	2.485813
428.115590	2038.737490	18.049370	-0.080424	2.481222
427.886331	2030.805239	18.054375	-0.080376	2.476624
427.718430	2022.857180	18.059379	-0.080340	2.472013
428.036942	2014.852491	18.064384	-0.080394	2.467398
427.643726	2006.929944	18.069389	-0.080316	2.462767
427.382301	1999.025587	18.074394	-0.080262	2.458149
427.534863	1991.016460	18.079399	-0.080285	2.453492
427.502398	1983.033743	18.084403	-0.080274	2.448828
427.279816	1975.094815	18.089408	-0.080227	2.444165
427.609643	1967.061149	18.094413	-0.080283	2.439481
427.700448	1959.136209	18.099418	-0.080295	2.434833
427.731626	1951.114196	18.104423	-0.080296	2.430115
427.399452	1943.213913	18.109427	-0.080229	2.425431
427.252465	1935.316081	18.114432	-0.080196	2.420753
427.563409	1927.265642	18.119437	-0.080249	2.416012
427.053421	1919.396826	18.124442	-0.080149	2.411305
427.044561	1911.399341	18.129447	-0.080142	2.406552
426.995518	1903.445028	18.134451	-0.080128	2.401812
427.126425	1895.484949	18.139456	-0.080147	2.397073
426.982663	1887.518928	18.144461	-0.080115	2.392300
427.378818	1879.509632	18.149466	-0.080184	2.387534
427.346996	1871.560128	18.154471	-0.080172	2.382760
426.967317	1863.677064	18.159475	-0.080097	2.377989
426.985343	1855.707231	18.164480	-0.080095	2.373188
427.067234	1847.702005	18.169485	-0.080105	2.368361
427.111365	1839.751649	18.174490	-0.080108	2.363554
426.701692	1831.897437	18.179495	-0.080026	2.358758
426.814044	1823.886977	18.184499	-0.080042	2.353901
426.842053	1815.931835	18.189504	-0.080042	2.349060
426.348236	1808.016271	18.194509	-0.079945	2.344190
426.531820	1800.043783	18.199514	-0.079974	2.339332
426.466809	1792.078120	18.204519	-0.079957	2.334447
426.245236	1784.142685	18.209523	-0.079910	2.329557
425.901614	1776.257227	18.214528	-0.079841	2.324677
425.466243	1768.342437	18.219533	-0.079755	2.319761
425.785417	1760.290925	18.224538	-0.079809	2.314814
425.391596	1752.391409	18.229543	-0.079731	2.309890
425.446040	1744.391004	18.234547	-0.079736	2.304930
425.543017	1736.431999	18.239552	-0.079749	2.299990
425.577960	1728.457037	18.244557	-0.079750	2.295024
425.284158	1720.558967	18.249562	-0.079690	2.290066
424.769371	1712.669403	18.254567	-0.079589	2.285084
424.850487	1704.668311	18.259571	-0.079599	2.280073
425.074042	1696.697965	18.264576	-0.079636	2.275082
425.680524	1688.581577	18.269581	-0.079743	2.270022
425.199768	1680.714421	18.274586	-0.079649	2.265013
425.532528	1672.710958	18.279591	-0.079705	2.259978
425.664345	1664.745506	18.284595	-0.079725	2.254938
425.615579	1656.831822	18.289600	-0.079710	2.249904
425.234410	1648.932696	18.294605	-0.079634	2.244838
425.611908	1640.954136	18.299610	-0.079699	2.239778
425.457962	1633.061076	18.304615	-0.079666	2.234713
425.149398	1625.144520	18.309619	-0.079603	2.229608
425.269804	1617.153198	18.314624	-0.079620	2.224482
424.871467	1609.293696	18.319629	-0.079541	2.219381
424.726573	1601.374278	18.324634	-0.079509	2.214254
424.697794	1593.408956	18.329639	-0.079498	2.209095
424.799629	1585.409162	18.334643	-0.079512	2.203914
424.637428	1577.524470	18.339648	-0.079477	2.198771
424.210794	1569.613323	18.344653	-0.079392	2.193574
424.431109	1561.617861	18.349658	-0.079428	2.188370
424.425546	1553.636240	18.354663	-0.079422	2.183141
423.738522	1545.823981	18.359667	-0.079289	2.177948
424.158380	1537.786262	18.364672	-0.079362	2.172697
423.928054	1529.844203	18.369677	-0.079314	2.167435
424.307743	1521.838819	18.374682	-0.079379	2.162177
423.578754	1514.047597	18.379687	-0.079238	2.156942
423.687364	1506.058103	18.384691	-0.079253	2.151643
423.926413	1498.054721	18.389696	-0.079293	2.146334
423.461412	1490.169607	18.394701	-0.079201	2.141023
423.626630	1482.212252	18.399706	-0.079227	2.135711
423.383621	1474.308319	18.404711	-0.079176	2.130382
423.276256	1466.355393	18.409715	-0.079151	2.125020
423.670056	1458.375114	18.414720	-0.079219	2.119675
423.819448	1450.418216	18.419725	-0.079242	2.114308
423.825110	1442.447954	18.424730	-0.079238	2.108904
423.423929	1434.577779	18.429735	-0.079158	2.103515
423.610190	1426.618672	18.434739	-0.079187	2.098109
423.011585	1418.799140	18.439744	-0.079071	2.092706
423.248129	1410.762719	18.444749	-0.079110	2.087224
423.353060	1402.836541	18.449754	-0.079124	2.081791
422.910407	1394.996235	18.454759	-0.079037	2.076347
422.673324	1387.083520	18.459763	-0.078987	2.070859
422.493317	1379.158583	18.464768	-0.078949	2.065355
422.354030	1371.216582	18.469773	-0.078917	2.059827
422.195398	1363.307557	18.474778	-0.078883	2.054306
421.757173	1355.429738	18.479783	-0.078796	2.048763
421.987047	1347.397891	18.484787	-0.078834	2.043166
422.232941	1339.452128	18.489792	-0.078874	2.037615
421.954748	1331.548231	18.494797	-0.078817	2.032025
421.753142	1323.649435	18.499802	-0.078775	2.026430
421.840835	1315.677994	18.504807	-0.078786	2.020799
421.288136	1307.849069	18.509811	-0.078678	2.015186
421.640078	1299.829258	18.514816	-0.078738	2.009517
421.891979	1291.844012	18.519821	-0.078780	2.003845
421.540660	1284.009227	18.524826	-0.078709	1.998202
421.345001	1276.117600	18.529831	-0.078668	1.992518
421.222148	1268.188593	18.534835	-0.078640	1.986799
421.450382	1260.220981	18.539840	-0.078677	1.981073
421.202129	1252.325912	18.544845	-0.078626	1.975331
421.263993	1244.391431	18.549850	-0.078632	1.969578
421.207420	1236.485179	18.554855	-0.078616	1.963815
420.941310	1228.609483	18.559859	-0.078562	1.958035
420.733868	1220.716277	18.564864	-0.078518	1.952232
420.614071	1212.767291	18.569869	-0.078491	1.946379
420.547466	1204.860284	18.574874	-0.078473	1.940546
420.780640	1196.873843	18.579879	-0.078511	1.934670
420.558877	1188.992574	18.584883	-0.078465	1.928803
420.368268	1181.110392	18.589888	-0.078424	1.922921
420.253744	1173.196836	18.594893	-0.078398	1.917006
420.135519	1165.300204	18.599898	-0.078371	1.911085
420.517749	1157.287113	18.604903	-0.078436	1.905115
420.176117	1149.454170	18.609907	-0.078368	1.899180
420.038615	1141.570939	18.614912	-0.078337	1.893211
420.079508	1133.617570	18.619917	-0.078340	1.887190
419.874988	1125.750134	18.624922	-0.078296	1.881187
420.061121	1117.805127	18.629927	-0.078326	1.875152
419.836578	1109.939773	18.634931	-0.078279	1.869109
419.967461	1101.994183	18.639936	-0.078298	1.863028
419.414853	1094.169096	18.644941	-0.078190	1.856938
419.367790	1086.247902	18.649946	-0.078176	1.850814
419.185267	1078.353245	18.654951	-0.078137	1.844674
419.441667	1070.407402	18.659955	-0.078180	1.838526
419.309705	1062.535943	18.664960	-0.078150	1.832369
419.798551	1054.511000	18.669965	-0.078236	1.826146
419.642842	1046.672439	18.674970	-0.078202	1.819970
419.467364	1038.823506	18.679975	-0.078164	1.813762
419.073557	1030.987303	18.684979	-0.078085	1.807516
419.154104	1023.081565	18.689984	-0.078095	1.801252
418.968906	1015.202801	18.694989	-0.078056	1.794955
418.663761	1007.334586	18.699994	-0.077994	1.788628
418.865268	999.368559	18.704999	-0.078026	1.782264
418.714499	991.495915	18.710003	-0.077993	1.775909
418.557838	983.629899	18.715008	-0.077959	1.769534
418.792604	975.667550	18.720013	-0.077997	1.763109
418.797765	967.810661	18.725018	-0.077993	1.756716
418.039354	960.057266	18.730023	-0.077847	1.750287
418.009260	952.138033	18.735027	-0.077836	1.743792
418.257595	944.221043	18.740032	-0.077877	1.737310
417.930070	936.362138	18.745037	-0.077811	1.730777
417.933218	928.481689	18.750042	-0.077807	1.724245
418.204483	920.555281	18.755047	-0.077852	1.717685
417.789413	912.753501	18.760051	-0.077770	1.711113
417.817051	904.851916	18.765056	-0.077770	1.704491
418.052300	896.923506	18.770061	-0.077808	1.697848
418.018257	889.062389	18.775066	-0.077797	1.691200
417.164193	881.332229	18.780071	-0.077633	1.684526
416.939158	873.487758	18.785075	-0.077586	1.677813
417.081222	865.573887	18.790080	-0.077607	1.671064
416.555351	857.751795	18.795085	-0.077504	1.664275
416.129827	849.943043	18.800090	-0.077420	1.657483
415.845032	842.091511	18.805095	-0.077362	1.650646
415.336912	834.280453	18.810099	-0.077262	1.643784
415.159955	826.427231	18.815104	-0.077224	1.636903
414.960642	818.502003	18.820109	-0.077182	1.629926
414.902601	810.611029	18.825114	-0.077166	1.622969
414.905869	802.718503	18.830119	-0.077161	1.615990
414.400969	794.923040	18.835123	-0.077062	1.608994
414.290156	787.064524	18.840128	-0.077036	1.601967
414.417910	779.159356	18.845133	-0.077055	1.594902
413.370454	771.488143	18.850138	-0.076855	1.587846
413.029608	763.640198	18.855143	-0.076786	1.580702
412.741266	755.806516	18.860147	-0.076728	1.573545
412.107119	748.029149	18.865152	-0.076604	1.566356
411.494525	740.246564	18.870157	-0.076485	1.559132
411.525003	732.357137	18.875162	-0.076486	1.551872
410.993199	724.538733	18.880167	-0.076382	1.544559
410.476990	716.740939	18.885171	-0.076281	1.537232
410.713667	708.808788	18.890176	-0.076319	1.529859
410.790978	700.914424	18.895181	-0.076329	1.522462
409.987015	693.211405	18.900186	-0.076174	1.515073
409.127357	685.515327	18.905191	-0.076009	1.507646
408.497222	677.729181	18.910195	-0.075887	1.500132
408.242428	669.906628	18.915200	-0.075834	1.492603
408.015023	662.035756	18.920205	-0.075787	1.484995
407.453463	654.298216	18.925210	-0.075677	1.477422
407.661027	646.352866	18.930215	-0.075710	1.469732
407.183335	638.561110	18.935219	-0.075616	1.462041
407.040528	630.749046	18.940224	-0.075585	1.454343
406.024284	623.074771	18.945229	-0.075391	1.446598
406.012438	615.234059	18.950234	-0.075383	1.438811
405.625166	607.454214	18.955239	-0.075306	1.430980
405.336962	599.648691	18.960243	-0.075247	1.423096
404.573772	591.965632	18.965248	-0.075100	1.415213
403.949896	584.210388	18.970253	-0.074979	1.407235
403.695349	576.421901	18.975258	-0.074927	1.399240
403.087106	568.691277	18.980263	-0.074808	1.391198
402.305159	560.978115	18.985267	-0.074658	1.383097
401.643016	553.257553	18.990272	-0.074529	1.374962
401.064196	545.496440	18.995277	-0.074417	1.366750
400.763068	537.723103	19.000282	-0.074355	1.358523
400.104139	530.004981	19.005287	-0.074228	1.350242
399.684597	522.238501	19.010291	-0.074145	1.341901
399.976681	514.381880	19.015296	-0.074194	1.333538
399.499299	506.636000	19.020301	-0.074100	1.325103
399.076963	498.941702	19.025306	-0.074016	1.316680
398.905865	491.098669	19.030311	-0.073979	1.308085
398.192898	483.415768	19.035315	-0.073842	1.299510
397.615483	475.739342	19.040320	-0.073729	1.290910
396.886371	468.080689	19.045325	-0.073588	1.282244
396.627872	460.358458	19.050330	-0.073535	1.273536
395.788595	452.729878	19.055335	-0.073374	1.264763
395.348170	445.031556	19.060339	-0.073287	1.255925
394.710713	437.383924	19.065344	-0.073163	1.247045
394.002963	429.737134	19.070349	-0.073027	1.238088
393.732139	422.018283	19.075354	-0.072971	1.229068
393.240590	414.338081	19.080359	-0.072875	1.219982
392.788678	406.665739	19.085363	-0.072785	1.210845
392.619418	398.956504	19.090368	-0.072749	1.201652
392.065880	391.329749	19.095373	-0.072641	1.192408
392.246949	383.566507	19.100378	-0.072670	1.183079
391.779378	375.951827	19.105383	-0.072578	1.173721
391.367662	368.329589	19.110387	-0.072496	1.164290
391.129289	360.695549	19.115392	-0.072447	1.154805
390.800084	353.047339	19.120397	-0.072380	1.145203
390.306893	345.469281	19.125402	-0.072284	1.135573
389.462008	337.953570	19.130407	-0.072121	1.125863
388.873037	330.405433	19.135411	-0.072007	1.116083
388.491701	322.815739	19.140416	-0.071931	1.106209
387.974867	315.263788	19.145421	-0.071830	1.096264
387.847175	307.639540	19.150426	-0.071801	1.086221
387.071209	300.171083	19.155431	-0.071652	1.076143
386.999875	292.544852	19.160435	-0.071633	1.065921
386.193618	285.115548	19.165440	-0.071478	1.055694
385.873204	277.553001	19.170445	-0.071414	1.045300
385.085448	270.129720	19.175450	-0.071262	1.034882
384.780987	262.604999	19.180455	-0.071201	1.024333
384.380651	255.114700	19.185459	-0.071121	1.013699
384.203465	247.596458	19.190464	-0.071083	1.002967
383.717138	240.153323	19.195469	-0.070988	0.992150
383.654892	232.625354	19.200474	-0.070972	0.981198
383.461530	225.155489	19.205479	-0.070931	0.970174
382.643749	217.837602	19.210483	-0.070774	0.959087
382.087379	210.480969	19.215488	-0.070665	0.947881
381.530003	203.112478	19.220493	-0.070557	0.936522
381.008883	195.774560	19.225498	-0.070455	0.925080
380.394848	188.471093	19.230503	-0.070336	0.913524
379.805190	181.156424	19.235507	-0.070221	0.901807
379.716387	173.783432	19.240512	-0.070200	0.889984
379.484307	166.462255	19.245517	-0.070152	0.878046
378.634327	159.286923	19.250522	-0.069989	0.866003
378.293771	152.022346	19.255527	-0.069921	0.853792
378.071517	144.768281	19.260531	-0.069875	0.841456
377.670923	137.576127	19.265536	-0.069796	0.828989
376.603959	130.515581	19.270541	-0.069592	0.816356
376.257836	123.344836	19.275546	-0.069523	0.803555
376.460203	116.113281	19.280551	-0.069556	0.790612
375.694534	109.101394	19.285555	-0.069409	0.777542
375.401165	102.030436	19.290560	-0.069350	0.764295
375.061601	94.999033	19.295565	-0.069282	0.750873
374.635716	88.019195	19.300570	-0.069198	0.737278
373.338871	81.232963	19.305575	-0.068952	0.723503
372.688146	74.539420	19.310579	-0.068827	0.709880