Mon Apr 19 09:32:36 2021

Number of Points = 3646
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
-0.325955	0.002957	0.000000	0.000005	0.311108

-0.082886	-0.039800	0.005005	-0.000040	0.311114
-0.873242	0.100471	0.010010	0.000107	0.311099
-1.125561	0.152138	0.015014	0.000154	0.311126
-0.307201	0.000155	0.020019	0.000002	0.311111
-0.370282	0.010443	0.025024	0.000013	0.311106
-0.660875	0.067310	0.030029	0.000067	0.311125
0.166253	-0.087718	0.035034	-0.000087	0.311103
0.037886	-0.060609	0.040038	-0.000063	0.311121
0.053257	-0.065787	0.045043	-0.000066	0.311110
0.348751	-0.139268	0.050048	-0.000121	0.311018
0.545288	-0.224058	0.055053	-0.000157	0.310789
-0.040337	-0.120556	0.060058	-0.000048	0.310776
-0.303552	-0.069488	0.065062	0.000001	0.310791
-0.013207	-0.124005	0.070067	-0.000053	0.310783
-0.709829	0.004308	0.075072	0.000076	0.310791
-1.159289	0.089334	0.080077	0.000160	0.310807
-0.554796	-0.024181	0.085082	0.000047	0.310790
-0.641358	-0.002613	0.090086	0.000064	0.310817
-1.280776	0.073191	0.095091	0.000182	0.310630
-0.691915	-0.050104	0.100096	0.000073	0.310554
-0.335454	-0.111660	0.105101	0.000007	0.310569
-0.426464	-0.097054	0.110106	0.000023	0.310560
-0.666420	-0.050126	0.115110	0.000068	0.310576
-0.521113	-0.077214	0.120115	0.000041	0.310573
-0.319936	-0.161094	0.125120	0.000004	0.310352
-0.872350	-0.088879	0.130125	0.000106	0.310221
-0.712286	-0.120012	0.135130	0.000077	0.310212
-0.463976	-0.165099	0.140134	0.000030	0.310212
-1.418502	0.010325	0.145139	0.000208	0.310221
-1.292059	-0.033495	0.150144	0.000184	0.310124
-0.775823	-0.172875	0.155149	0.000088	0.309912
-0.589296	-0.211945	0.160154	0.000054	0.309887
-0.587163	-0.211106	0.165158	0.000053	0.309893
-0.172382	-0.301282	0.170163	-0.000024	0.309824
0.052609	-0.399764	0.175168	-0.000066	0.309555
-0.540650	-0.289570	0.180173	0.000044	0.309567
-0.887858	-0.225370	0.185178	0.000109	0.309572
0.186308	-0.472332	0.190182	-0.000091	0.309330
-0.587191	-0.340918	0.195187	0.000053	0.309287
-0.366807	-0.386517	0.200192	0.000012	0.309262
0.231894	-0.546151	0.205197	-0.000099	0.309024
-0.248432	-0.478798	0.210202	-0.000010	0.308931
-0.472631	-0.438840	0.215206	0.000032	0.308927
0.181437	-0.620106	0.220211	-0.000090	0.308635
0.075925	-0.605275	0.225216	-0.000070	0.308614
-0.347426	-0.550905	0.230221	0.000008	0.308509
-0.219184	-0.620003	0.235226	-0.000016	0.308294
0.374087	-0.727237	0.240230	-0.000126	0.308297
0.146607	-0.743903	0.245235	-0.000084	0.308025
-0.699651	-0.597568	0.250240	0.000074	0.307990
-0.762983	-0.609200	0.255245	0.000086	0.307881
-0.985299	-0.611613	0.260250	0.000127	0.307680
-1.259907	-0.563222	0.265254	0.000178	0.307673
-0.865004	-0.694553	0.270259	0.000105	0.307393
-0.081082	-0.850117	0.275264	-0.000041	0.307332
-0.221906	-0.860666	0.280269	-0.000015	0.307161
-0.749526	-0.795059	0.285274	0.000083	0.307019
-0.200774	-0.916728	0.290278	-0.000019	0.306916
0.186264	-1.026045	0.295283	-0.000091	0.306732
0.413403	-1.102039	0.300288	-0.000133	0.306568
0.589409	-1.172497	0.305293	-0.000166	0.306387
0.273693	-1.155464	0.310298	-0.000107	0.306196
-0.359885	-1.062242	0.315302	0.000011	0.306093
-1.103447	-0.973413	0.320307	0.000149	0.305874
-0.743348	-1.060031	0.325312	0.000082	0.305774
-0.971468	-1.052687	0.330317	0.000124	0.305613
-1.646663	-0.949931	0.335322	0.000250	0.305519
-1.272741	-1.057804	0.340326	0.000180	0.305330
-0.629390	-1.206895	0.345331	0.000061	0.305177
-1.090864	-1.169741	0.350336	0.000147	0.304956
-0.761552	-1.247735	0.355341	0.000085	0.304870
-0.494064	-1.354994	0.360346	0.000035	0.304591
-0.176919	-1.433421	0.365350	-0.000024	0.304493
-0.106331	-1.497646	0.370355	-0.000037	0.304249
-0.611901	-1.444294	0.375360	0.000057	0.304066
-0.923160	-1.416841	0.380365	0.000115	0.303927
-1.302317	-1.404772	0.385370	0.000186	0.303657
-1.720881	-1.338936	0.390374	0.000264	0.303608
-1.444932	-1.457120	0.395379	0.000212	0.303284
-1.577335	-1.452124	0.400384	0.000237	0.303193
-1.279113	-1.545162	0.405389	0.000182	0.303008
-1.255192	-1.595779	0.410394	0.000177	0.302787
-2.093413	-1.468612	0.415398	0.000333	0.302667
-1.827496	-1.577904	0.420403	0.000284	0.302375
-0.879358	-1.777853	0.425408	0.000107	0.302243
-0.642908	-1.866283	0.430413	0.000063	0.302025
-1.540202	-1.751503	0.435418	0.000230	0.301794
-1.918178	-1.709988	0.440422	0.000300	0.301664
-1.195522	-1.900907	0.445427	0.000166	0.301378
-1.021169	-1.978000	0.450432	0.000134	0.301160
-1.371054	-1.945897	0.455437	0.000199	0.301009
-1.664693	-1.945082	0.460442	0.000253	0.300757
-2.067912	-1.905334	0.465446	0.000328	0.300595
-1.650925	-2.010027	0.470451	0.000251	0.300456
-1.540781	-2.086264	0.475456	0.000230	0.300186
-2.294215	-1.997067	0.480461	0.000370	0.299956
-2.657415	-1.965224	0.485466	0.000438	0.299791
-2.936904	-1.963194	0.490470	0.000490	0.299556
-2.549364	-2.077218	0.495475	0.000418	0.299345
-2.683015	-2.086329	0.500480	0.000443	0.299184
-3.058942	-2.070671	0.505485	0.000513	0.298929
-2.969237	-2.132579	0.510490	0.000496	0.298708
-3.646408	-2.037764	0.515494	0.000622	0.298572
-3.483645	-2.127085	0.520499	0.000592	0.298282
-3.637400	-2.131211	0.525504	0.000620	0.298127
-3.997178	-2.092650	0.530509	0.000687	0.297997
-4.842821	-2.007882	0.535514	0.000845	0.297662
-4.404873	-2.107753	0.540518	0.000763	0.297563
-5.358437	-1.975384	0.545523	0.000941	0.297364
-5.461653	-1.996988	0.550528	0.000960	0.297168
-5.543068	-2.010491	0.555533	0.000975	0.297030
-5.316126	-2.103603	0.560538	0.000933	0.296778
-5.312526	-2.124940	0.565542	0.000932	0.296677
-5.770315	-2.100245	0.570547	0.001017	0.296392
-6.164112	-2.052088	0.575552	0.001090	0.296277
-6.681472	-1.995020	0.580557	0.001187	0.296097
-6.439157	-2.078900	0.585562	0.001142	0.295902
-5.848739	-2.218703	0.590566	0.001032	0.295744
-6.271988	-2.182137	0.595571	0.001111	0.295546
-6.637174	-2.134724	0.600576	0.001178	0.295453
-6.207606	-2.273083	0.605581	0.001099	0.295158
-6.525649	-2.246066	0.610586	0.001158	0.295007
-7.330053	-2.133967	0.615590	0.001307	0.294840
-7.241773	-2.194899	0.620595	0.001291	0.294620
-7.439106	-2.181163	0.625600	0.001328	0.294511
-7.362706	-2.245952	0.630605	0.001313	0.294261
-8.061910	-2.132585	0.635610	0.001444	0.294194
-8.254107	-2.158497	0.640614	0.001479	0.293895
-8.188746	-2.184967	0.645619	0.001467	0.293823
-8.370286	-2.203816	0.650624	0.001501	0.293568
-7.724311	-2.348272	0.655629	0.001381	0.293434
-8.687925	-2.211193	0.660634	0.001560	0.293247
-8.768783	-2.232242	0.665638	0.001575	0.293070
-9.012974	-2.210478	0.670643	0.001621	0.292959
-9.030523	-2.259685	0.675648	0.001624	0.292700
-9.481915	-2.191778	0.680653	0.001708	0.292630
-9.993055	-2.152773	0.685658	0.001803	0.292364
-9.913679	-2.177036	0.690662	0.001788	0.292315
-10.285564	-2.158157	0.695667	0.001857	0.292074
-11.040511	-2.035197	0.700672	0.001998	0.292003
-11.018858	-2.076134	0.705677	0.001994	0.291820
-11.062730	-2.089863	0.710682	0.002002	0.291713
-11.035112	-2.128232	0.715686	0.001997	0.291547
-11.941050	-1.991263	0.720691	0.002165	0.291410
-11.961911	-2.000098	0.725696	0.002169	0.291347
-11.787933	-2.082439	0.730701	0.002137	0.291095
-11.947071	-2.056921	0.735706	0.002166	0.291078
-11.869498	-2.133289	0.740710	0.002152	0.290769
-12.128828	-2.088233	0.745715	0.002200	0.290759
-12.683486	-2.024222	0.750720	0.002303	0.290575
-12.185688	-2.127530	0.755725	0.002211	0.290512
-12.464716	-2.111556	0.760730	0.002263	0.290339
-12.992659	-2.050927	0.765734	0.002361	0.290163
-12.708579	-2.117401	0.770739	0.002308	0.290089
-13.191120	-2.079721	0.775744	0.002398	0.289839
-12.808532	-2.148581	0.780749	0.002327	0.289843
-13.413007	-2.106716	0.785754	0.002439	0.289503
-13.360332	-2.114683	0.790758	0.002429	0.289511
-13.112185	-2.201439	0.795763	0.002383	0.289303
-13.513662	-2.148364	0.800768	0.002458	0.289204
-13.546397	-2.174249	0.805773	0.002464	0.289044
-14.026114	-2.121423	0.810778	0.002553	0.288872
-13.999979	-2.140357	0.815782	0.002548	0.288801
-14.660625	-2.062465	0.820787	0.002671	0.288590
-14.746028	-2.048259	0.825792	0.002687	0.288583
-14.410233	-2.163309	0.830797	0.002625	0.288313
-15.367692	-1.999484	0.835802	0.002803	0.288261
-14.963896	-2.098773	0.840806	0.002728	0.288132
-14.983569	-2.128905	0.845811	0.002731	0.287962
-14.930318	-2.147906	0.850816	0.002721	0.287916
-15.366480	-2.125247	0.855821	0.002802	0.287631
-15.538128	-2.096090	0.860826	0.002834	0.287621
-15.799621	-2.089609	0.865830	0.002883	0.287414
-15.734169	-2.123556	0.870835	0.002871	0.287303
-16.074862	-2.077428	0.875840	0.002934	0.287224
-15.824927	-2.169338	0.880845	0.002888	0.286990
-16.358074	-2.074316	0.885850	0.002987	0.286980
-16.416819	-2.110648	0.890854	0.002998	0.286743
-16.224350	-2.154197	0.895859	0.002962	0.286700
-16.743224	-2.091235	0.900864	0.003059	0.286542
-16.794329	-2.117453	0.905869	0.003068	0.286363
-16.480402	-2.178552	0.910874	0.003010	0.286342
-17.098435	-2.123451	0.915878	0.003125	0.286053
-17.230653	-2.100115	0.920883	0.003149	0.286049
-17.725014	-2.040391	0.925888	0.003241	0.285897
-17.765400	-2.060308	0.930893	0.003249	0.285759
-18.241500	-1.976119	0.935898	0.003337	0.285747
-18.315607	-2.004296	0.940902	0.003351	0.285536
-17.561371	-2.151483	0.945907	0.003211	0.285485
-18.219149	-2.054624	0.950912	0.003333	0.285370
-18.370849	-2.071553	0.955917	0.003361	0.285145
-18.647823	-2.019087	0.960922	0.003413	0.285155
-18.544233	-2.081009	0.965926	0.003394	0.284937
-19.277496	-1.965193	0.970931	0.003530	0.284848
-18.725658	-2.072304	0.975936	0.003427	0.284814
-18.665999	-2.142686	0.980941	0.003416	0.284511
-19.088838	-2.069913	0.985946	0.003495	0.284490
-19.365594	-2.048088	0.990950	0.003546	0.284346
-19.460430	-2.053699	0.995955	0.003564	0.284229
-19.520775	-2.046816	1.000960	0.003575	0.284209
-19.593886	-2.089984	1.005965	0.003589	0.283921
-19.914591	-2.039709	1.010970	0.003648	0.283880
-19.950532	-2.049299	1.015974	0.003655	0.283798
-20.098634	-2.066898	1.020979	0.003683	0.283571
-20.654710	-1.964464	1.025984	0.003786	0.283578
-20.142432	-2.093890	1.030989	0.003691	0.283393
-20.731177	-2.014216	1.035994	0.003800	0.283253
-20.600157	-2.038504	1.040998	0.003776	0.283251
-20.481965	-2.112731	1.046003	0.003754	0.282982
-20.549814	-2.107963	1.051008	0.003766	0.282943
-20.727987	-2.100438	1.056013	0.003800	0.282816
-21.165659	-2.060036	1.061018	0.003881	0.282615
-20.913362	-2.106621	1.066022	0.003834	0.282612
-21.047255	-2.132633	1.071027	0.003859	0.282354
-21.646897	-2.034449	1.076032	0.003971	0.282299
-21.389318	-2.094893	1.081037	0.003923	0.282229
-21.813663	-2.065201	1.086042	0.004002	0.281985
-21.721861	-2.082551	1.091046	0.003984	0.281982
-21.660520	-2.130111	1.096051	0.003973	0.281795
-21.893558	-2.109851	1.101056	0.004016	0.281682
-22.116888	-2.071576	1.106061	0.004058	0.281670
-22.397305	-2.081510	1.111066	0.004110	0.281357
-21.999751	-2.154274	1.116070	0.004036	0.281355
-22.302626	-2.132577	1.121075	0.004092	0.281183
-23.286947	-1.977615	1.126080	0.004276	0.281060
-22.435607	-2.132181	1.131085	0.004117	0.281061
-23.035690	-2.080248	1.136090	0.004229	0.280766
-23.915491	-1.921926	1.141094	0.004393	0.280758
-23.475269	-2.007288	1.146099	0.004311	0.280731
-23.334976	-2.076510	1.151104	0.004285	0.280505
-23.607052	-2.025644	1.156109	0.004335	0.280513
-23.904652	-2.000744	1.161114	0.004390	0.280362
-23.810732	-2.056186	1.166118	0.004373	0.280164
-23.504721	-2.112316	1.171123	0.004316	0.280162
-24.159286	-2.044702	1.176128	0.004438	0.279896
-23.982297	-2.087248	1.181133	0.004405	0.279843
-24.042055	-2.088954	1.186138	0.004416	0.279778
-24.301729	-2.093178	1.191142	0.004464	0.279512
-24.060371	-2.137612	1.196147	0.004419	0.279509
-24.373237	-2.118878	1.201152	0.004478	0.279311
-24.924767	-2.033310	1.206157	0.004580	0.279235
-24.987706	-2.024328	1.211162	0.004592	0.279223
-24.864422	-2.110329	1.216166	0.004569	0.278893
-25.045813	-2.076188	1.221171	0.004603	0.278899
-25.369416	-2.041768	1.226176	0.004663	0.278772
-25.565356	-2.040772	1.231181	0.004699	0.278593
-25.017678	-2.143858	1.236186	0.004597	0.278574
-25.819374	-2.043831	1.241190	0.004747	0.278337
-26.168558	-1.993041	1.246195	0.004812	0.278271
-25.509741	-2.120234	1.251200	0.004689	0.278233
-25.548691	-2.163089	1.256205	0.004696	0.277973
-26.255274	-2.035035	1.261210	0.004828	0.277971
-26.364109	-2.045891	1.266214	0.004848	0.277811
-26.441867	-2.065693	1.271219	0.004862	0.277634
-26.843811	-1.993325	1.276224	0.004937	0.277631
-26.501845	-2.101282	1.281229	0.004873	0.277392
-26.803264	-2.061253	1.286234	0.004930	0.277315
-26.914878	-2.049045	1.291238	0.004950	0.277273
-27.345738	-2.021803	1.296243	0.005030	0.277006
-26.948438	-2.098670	1.301248	0.004957	0.276982
-26.755976	-2.160964	1.306253	0.004921	0.276840
-27.423865	-2.068275	1.311258	0.005045	0.276689
-27.118792	-2.122101	1.316262	0.004988	0.276698
-27.567444	-2.099466	1.321267	0.005072	0.276390
-27.786188	-2.065128	1.326272	0.005112	0.276361
-27.746366	-2.089357	1.331277	0.005105	0.276272
-27.884916	-2.105582	1.336282	0.005131	0.276055
-27.837850	-2.113075	1.341286	0.005122	0.276061
-28.207183	-2.091494	1.346291	0.005191	0.275822
-28.317175	-2.085974	1.351296	0.005211	0.275746
-28.065000	-2.140685	1.356301	0.005164	0.275700
-28.789646	-2.046669	1.361306	0.005299	0.275502
-28.421607	-2.114832	1.366310	0.005230	0.275495
-28.417614	-2.155030	1.371315	0.005230	0.275288
-28.914113	-2.090535	1.376320	0.005322	0.275152
-29.015887	-2.075384	1.381325	0.005341	0.275135
-29.167279	-2.101617	1.386330	0.005369	0.274852
-29.378691	-2.064220	1.391334	0.005409	0.274846
-29.556849	-2.059359	1.396339	0.005442	0.274702
-29.754715	-2.058208	1.401344	0.005478	0.274518
-29.404729	-2.120140	1.406349	0.005413	0.274527
-30.136673	-2.035000	1.411354	0.005550	0.274274
-30.173009	-2.036677	1.416358	0.005556	0.274231
-29.529157	-2.167837	1.421363	0.005436	0.274157
-30.125107	-2.112354	1.426368	0.005547	0.273877
-30.302878	-2.075626	1.431373	0.005580	0.273901
-30.769485	-2.026228	1.436378	0.005667	0.273713
-30.616890	-2.077200	1.441382	0.005639	0.273591
-30.756262	-2.051402	1.446387	0.005665	0.273593
-31.094895	-2.047174	1.451392	0.005728	0.273289
-31.099593	-2.046402	1.456397	0.005729	0.273289
-31.581992	-1.972251	1.461402	0.005818	0.273217
-31.410218	-2.048052	1.466406	0.005786	0.272981
-31.211295	-2.082909	1.471411	0.005749	0.272988
-31.449843	-2.079087	1.476416	0.005794	0.272779
-31.685087	-2.060960	1.481421	0.005837	0.272648
-31.799306	-2.039917	1.486426	0.005859	0.272650
-32.492821	-1.964700	1.491430	0.005988	0.272379
-32.786788	-1.915273	1.496435	0.006042	0.272358
-33.241050	-1.831660	1.501440	0.006127	0.272363
-32.497890	-2.019855	1.506445	0.005989	0.272081
-33.542369	-1.838841	1.511450	0.006183	0.272034
-33.275572	-1.886943	1.516454	0.006133	0.272036
-33.146872	-1.955943	1.521459	0.006109	0.271794
-33.418891	-1.919401	1.526464	0.006160	0.271725
-32.805112	-2.032704	1.531469	0.006046	0.271716
-33.255307	-2.010819	1.536474	0.006129	0.271396
-33.224743	-2.017181	1.541478	0.006124	0.271392
-34.047671	-1.874756	1.546483	0.006277	0.271354
-33.995793	-1.933769	1.551488	0.006267	0.271089
-33.806988	-1.965288	1.556493	0.006232	0.271104
-34.260934	-1.903038	1.561498	0.006317	0.270996
-34.306304	-1.936064	1.566502	0.006325	0.270776
-33.735569	-2.039805	1.571507	0.006219	0.270776
-34.144323	-1.996096	1.576512	0.006295	0.270612
-34.686220	-1.911932	1.581517	0.006396	0.270535
-34.273982	-1.990471	1.586522	0.006319	0.270517
-34.419670	-2.016574	1.591526	0.006346	0.270235
-34.915724	-1.935123	1.596531	0.006438	0.270188
-34.741240	-1.976776	1.601536	0.006406	0.270135
-34.704214	-2.034821	1.606541	0.006399	0.269860
-35.822920	-1.829060	1.611546	0.006607	0.269873
-35.521589	-1.899128	1.616550	0.006551	0.269791
-35.944583	-1.864426	1.621555	0.006630	0.269564
-36.141232	-1.830950	1.626560	0.006666	0.269552
-35.946781	-1.877505	1.631565	0.006630	0.269492
-36.143184	-1.884451	1.636570	0.006667	0.269263
-35.454194	-2.013156	1.641574	0.006538	0.269245
-36.089125	-1.922718	1.646579	0.006656	0.269110
-36.684263	-1.851964	1.651584	0.006767	0.268908
-35.678443	-2.035078	1.656589	0.006580	0.268908
-36.004867	-2.016121	1.661594	0.006641	0.268690
-36.852684	-1.877413	1.666598	0.006799	0.268607
-36.550979	-1.930943	1.671603	0.006742	0.268614
-36.623604	-1.978288	1.676608	0.006756	0.268288
-36.666396	-1.972990	1.681613	0.006764	0.268274
-36.686966	-1.984391	1.686618	0.006768	0.268193
-36.547606	-2.048962	1.691622	0.006742	0.267981
-36.717547	-2.017111	1.696627	0.006773	0.267986
-37.019847	-2.013586	1.701632	0.006830	0.267708
-36.778802	-2.069641	1.706637	0.006785	0.267642
-36.814739	-2.084488	1.711642	0.006791	0.267527
-37.670845	-1.966952	1.716646	0.006951	0.267320
-37.392908	-2.016658	1.721651	0.006899	0.267325
-37.520795	-2.038772	1.726656	0.006923	0.267079
-37.923374	-1.978068	1.731661	0.006998	0.267011
-38.193498	-1.934668	1.736666	0.007048	0.266980
-37.828095	-2.048885	1.741670	0.006980	0.266721
-37.840446	-2.046949	1.746675	0.006982	0.266720
-38.443953	-1.976731	1.751680	0.007094	0.266505
-38.107128	-2.060557	1.756685	0.007032	0.266383
-38.161498	-2.055910	1.761690	0.007042	0.266354
-38.936792	-1.965619	1.766694	0.007186	0.266079
-38.661113	-2.015698	1.771699	0.007135	0.266079
-38.903239	-2.001912	1.776704	0.007180	0.265915
-39.124347	-1.990341	1.781709	0.007221	0.265759
-39.467938	-1.926312	1.786714	0.007285	0.265767
-39.626362	-1.934485	1.791718	0.007314	0.265566
-39.270609	-2.010519	1.796723	0.007248	0.265504
-39.674775	-1.951033	1.801728	0.007323	0.265428
-39.784522	-1.976235	1.806733	0.007344	0.265181
-39.984350	-1.942111	1.811738	0.007381	0.265169
-40.136095	-1.949641	1.816742	0.007409	0.264977
-40.191369	-1.963608	1.821747	0.007419	0.264846
-39.829579	-2.031778	1.826752	0.007352	0.264834
-40.024688	-2.052798	1.831757	0.007388	0.264525
-40.671637	-1.938177	1.836762	0.007509	0.264508
-40.564567	-1.976302	1.841766	0.007489	0.264406
-40.714816	-1.979320	1.846771	0.007517	0.264240
-41.292287	-1.873898	1.851776	0.007624	0.264242
-41.154572	-1.939880	1.856781	0.007599	0.264018
-41.149084	-1.963696	1.861786	0.007597	0.263893
-41.099213	-1.977164	1.866790	0.007588	0.263869
-41.030970	-2.043125	1.871795	0.007575	0.263575
-41.638355	-1.929494	1.876800	0.007688	0.263592
-41.645920	-1.955100	1.881805	0.007690	0.263444
-41.804621	-1.960893	1.886810	0.007719	0.263254
-41.066741	-2.096519	1.891814	0.007582	0.263246
-41.235940	-2.115667	1.896819	0.007614	0.262971
-41.982010	-1.984002	1.901824	0.007752	0.262949
-41.643692	-2.077164	1.906829	0.007689	0.262775
-41.904998	-2.058896	1.911834	0.007738	0.262614
-42.487457	-1.954139	1.916838	0.007846	0.262608
-42.744198	-1.960123	1.921843	0.007894	0.262317
-42.871122	-1.937383	1.926848	0.007918	0.262315
-42.623317	-2.006710	1.931853	0.007872	0.262181
-43.502221	-1.878450	1.936858	0.008035	0.262007
-43.249253	-1.925685	1.941862	0.007988	0.262000
-43.172175	-1.972911	1.946867	0.007974	0.261817
-43.677943	-1.900438	1.951872	0.008068	0.261709
-43.134912	-2.006302	1.956877	0.007967	0.261670
-43.444965	-2.003465	1.961882	0.008024	0.261373
-43.219470	-2.047904	1.966886	0.007982	0.261355
-43.073419	-2.109576	1.971891	0.007955	0.261160
-43.595318	-2.035677	1.976896	0.008052	0.261044
-43.721439	-2.025332	1.981901	0.008076	0.260974
-44.284031	-1.966328	1.986906	0.008181	0.260733
-44.141623	-1.992174	1.991910	0.008154	0.260734
-43.912198	-2.062664	1.996915	0.008111	0.260574
-44.515177	-1.969854	2.001920	0.008223	0.260481

-44.560709	-2.019406	2.011917	0.008232	0.260159
-44.844064	-2.003947	2.021914	0.008285	0.259958
-44.870221	-2.020471	2.031910	0.008289	0.259840
-45.099539	-2.032913	2.041907	0.008332	0.259538
-45.299295	-2.001885	2.051904	0.008369	0.259509
-45.447307	-2.021712	2.061901	0.008397	0.259248
-45.806762	-1.959093	2.071898	0.008464	0.259233
-45.792227	-1.968254	2.081894	0.008461	0.259197
-46.071779	-1.971211	2.091891	0.008513	0.258896
-45.794844	-2.024074	2.101888	0.008461	0.258883
-46.087125	-1.969055	2.111885	0.008516	0.258893
-46.124533	-1.962073	2.121882	0.008522	0.258895
-45.738450	-2.034804	2.131878	0.008451	0.258881
-46.109719	-2.010659	2.141875	0.008520	0.258638
-46.569364	-1.937229	2.151872	0.008605	0.258582
-46.124024	-2.021153	2.161869	0.008522	0.258566
-46.424357	-1.953116	2.171866	0.008578	0.258641
-45.695407	-2.041876	2.181862	0.008442	0.258887
-45.937468	-1.997924	2.191859	0.008487	0.258887
-45.957610	-1.994111	2.201856	0.008491	0.258888
-45.793098	-2.024807	2.211853	0.008460	0.258884
-45.851756	-2.015276	2.221850	0.008471	0.258878
-45.533511	-2.074174	2.231846	0.008412	0.258872
-45.887028	-2.006593	2.241843	0.008478	0.258891
-45.944011	-1.973505	2.251840	0.008488	0.259018
-45.913481	-1.939555	2.261837	0.008482	0.259239
-45.854246	-1.950910	2.271834	0.008471	0.259237
-45.601782	-1.991512	2.281830	0.008424	0.259267
-45.410530	-1.981676	2.291827	0.008389	0.259516
-45.414538	-1.982139	2.301824	0.008389	0.259510
-45.176959	-2.012299	2.311821	0.008345	0.259583
-44.927159	-2.013193	2.321818	0.008298	0.259832
-44.726406	-2.049888	2.331814	0.008261	0.259831
-44.931227	-1.978817	2.341811	0.008299	0.260020
-44.736900	-1.989383	2.351808	0.008263	0.260158
-44.640242	-1.990246	2.361805	0.008245	0.260251
-44.341846	-2.001056	2.371802	0.008189	0.260494
-44.169729	-2.028855	2.381798	0.008157	0.260513
-44.197622	-1.984381	2.391795	0.008162	0.260733
-44.105722	-1.995349	2.401792	0.008145	0.260765
-44.045446	-1.953848	2.411789	0.008134	0.261056
-43.857986	-1.975353	2.421786	0.008099	0.261127
-43.282029	-2.037146	2.431782	0.007992	0.261365
-43.610871	-1.950242	2.441779	0.008053	0.261515
-42.927901	-2.041877	2.451776	0.007925	0.261696
-43.336394	-1.935006	2.461773	0.008001	0.261877
-43.328857	-1.913774	2.471770	0.008000	0.262002
-42.816856	-1.948758	2.481766	0.007905	0.262324
-42.823057	-1.925951	2.491763	0.007906	0.262444
-42.255253	-1.994840	2.501760	0.007800	0.262634
-42.274727	-1.942319	2.511757	0.007803	0.262904
-42.043295	-1.962240	2.521754	0.007760	0.263026
-42.049489	-1.917147	2.531750	0.007761	0.263269
-41.491737	-1.979025	2.541747	0.007658	0.263486
-41.506420	-1.949855	2.551744	0.007660	0.263632
-41.453231	-1.912568	2.561741	0.007650	0.263891
-40.564698	-2.035201	2.571738	0.007485	0.264105
-40.633975	-1.995385	2.581734	0.007498	0.264254
-40.320140	-2.006426	2.591731	0.007439	0.264507
-40.254107	-1.983340	2.601728	0.007427	0.264699
-40.229398	-1.957371	2.611725	0.007422	0.264866
-39.825381	-1.977210	2.621722	0.007347	0.265160
-39.609663	-1.977884	2.631718	0.007307	0.265370
-39.308382	-2.001780	2.641715	0.007250	0.265539
-38.971292	-2.024271	2.651712	0.007188	0.265751
-39.066653	-1.966774	2.661709	0.007205	0.265970
-38.831839	-1.974857	2.671706	0.007162	0.266159
-38.560018	-1.983037	2.681702	0.007111	0.266384
-38.136444	-2.006869	2.691699	0.007032	0.266673
-37.937553	-2.013621	2.701696	0.006995	0.266833
-37.791357	-2.010467	2.711693	0.006968	0.266995
-37.690291	-1.968478	2.721690	0.006949	0.267322
-37.624706	-1.942854	2.731686	0.006936	0.267526
-37.022809	-2.014830	2.741683	0.006824	0.267729
-36.843067	-2.001076	2.751680	0.006791	0.267981
-36.581760	-2.005131	2.761677	0.006742	0.268216
-36.679349	-1.951777	2.771674	0.006760	0.268408
-36.383748	-1.964052	2.781670	0.006705	0.268632
-35.891320	-2.003264	2.791667	0.006613	0.268904
-35.576715	-2.015216	2.801664	0.006555	0.269148
-36.266370	-1.849578	2.811661	0.006683	0.269364
-35.867437	-1.876190	2.821658	0.006609	0.269611
-35.395947	-1.914077	2.831654	0.006521	0.269869
-34.853850	-1.958646	2.841651	0.006420	0.270159
-34.578786	-1.966108	2.851648	0.006369	0.270387
-34.401138	-1.962778	2.861645	0.006335	0.270578
-34.449175	-1.916853	2.871642	0.006344	0.270777
-34.337916	-1.877535	2.881638	0.006324	0.271096
-33.929411	-1.907319	2.891635	0.006247	0.271334
-33.908247	-1.863509	2.901632	0.006243	0.271588
-33.344526	-1.927393	2.911629	0.006138	0.271794
-32.279509	-2.082687	2.921626	0.005940	0.271999
-32.798883	-1.933123	2.931622	0.006037	0.272293
-32.510155	-1.945291	2.941619	0.005983	0.272507
-31.923714	-2.013860	2.951616	0.005874	0.272710
-31.582469	-2.024283	2.961613	0.005810	0.272984
-31.635400	-1.968744	2.971610	0.005820	0.273228
-31.582837	-1.939807	2.981606	0.005810	0.273432
-30.794601	-2.045725	2.991603	0.005663	0.273631
-31.097050	-1.937481	3.001600	0.005719	0.273912
-30.657567	-1.964587	3.011597	0.005638	0.274192
-30.428780	-1.967175	3.021594	0.005595	0.274398
-30.479536	-1.916236	3.031590	0.005604	0.274618
-29.758160	-2.001420	3.041587	0.005470	0.274861
-29.735468	-1.952135	3.051584	0.005466	0.275142
-29.408016	-1.965933	3.061581	0.005405	0.275383
-29.518914	-1.904152	3.071578	0.005425	0.275602
-29.125014	-1.941164	3.081574	0.005352	0.275784
-28.543926	-1.990513	3.091571	0.005244	0.276080
-28.440967	-1.968593	3.101568	0.005224	0.276294
-27.901600	-2.029465	3.111565	0.005124	0.276489
-27.986634	-1.969575	3.121562	0.005140	0.276722
-27.342103	-2.034396	3.131558	0.005020	0.276996
-27.275136	-2.004194	3.141555	0.005007	0.277217
-27.488464	-1.921527	3.151552	0.005047	0.277447
-26.654405	-2.035812	3.161549	0.004891	0.277642
-26.394924	-2.020384	3.171546	0.004843	0.277969
-25.924431	-2.073301	3.181542	0.004755	0.278139
-25.725282	-2.074812	3.191539	0.004718	0.278320
-25.429269	-2.079374	3.201536	0.004663	0.278576
-24.955077	-2.120937	3.211533	0.004575	0.278808
-25.214358	-2.039926	3.221530	0.004623	0.278984
-24.830464	-2.062391	3.231526	0.004551	0.279230
-24.389359	-2.093949	3.241523	0.004469	0.279483
-24.492888	-2.039068	3.251520	0.004488	0.279670
-24.042421	-2.083160	3.261517	0.004405	0.279866
-24.091893	-2.016949	3.271514	0.004414	0.280162
-23.633529	-2.051771	3.281510	0.004328	0.280412
-23.948108	-1.955263	3.291507	0.004387	0.280616
-23.605171	-1.982659	3.301504	0.004323	0.280796
-23.516424	-1.945679	3.311501	0.004306	0.281070
-23.646931	-1.864981	3.321498	0.004330	0.281364
-23.013644	-1.928516	3.331494	0.004212	0.281629
-22.562451	-1.968334	3.341491	0.004128	0.281847
-22.294292	-1.979602	3.351488	0.004078	0.282039
-22.216897	-1.938716	3.361485	0.004064	0.282322
-21.823276	-1.954181	3.371482	0.003991	0.282609
-21.306905	-2.002527	3.381478	0.003894	0.282843
-21.120914	-1.994273	3.391475	0.003860	0.283058
-20.881628	-1.998399	3.401472	0.003815	0.283260
-20.360718	-2.034115	3.411469	0.003718	0.283561
-20.258206	-2.013918	3.421466	0.003699	0.283760
-19.915487	-2.035301	3.431462	0.003635	0.283969
-19.664782	-2.032536	3.441459	0.003588	0.284215
-19.313916	-2.048818	3.451456	0.003523	0.284458
-19.169783	-2.035250	3.461453	0.003496	0.284660
-18.841112	-2.058022	3.471450	0.003435	0.284848
-18.520495	-2.056635	3.481446	0.003375	0.285152
-18.514694	-2.011655	3.491443	0.003374	0.285386
-18.057789	-2.058871	3.501440	0.003289	0.285568
-18.309498	-1.976840	3.511437	0.003336	0.285752
-17.588377	-2.047174	3.521434	0.003201	0.286060
-17.321010	-2.060382	3.531430	0.003151	0.286239
-17.609173	-1.960734	3.541427	0.003205	0.286478
-16.758474	-2.070407	3.551424	0.003047	0.286706
-16.676112	-2.033953	3.561421	0.003031	0.286965
-16.285728	-2.069732	3.571418	0.002959	0.287143
-15.934705	-2.093570	3.581414	0.002893	0.287345
-15.755552	-2.070730	3.591411	0.002860	0.287624
-15.532632	-2.063618	3.601408	0.002818	0.287864
-15.308396	-2.068904	3.611405	0.002776	0.288042
-15.047967	-2.075047	3.621402	0.002728	0.288250
-14.873122	-2.048688	3.631398	0.002695	0.288542
-14.524021	-2.076125	3.641395	0.002630	0.288723
-14.276426	-2.082153	3.651392	0.002584	0.288918
-14.355522	-2.006135	3.661389	0.002599	0.289227
-13.616409	-2.098738	3.671386	0.002461	0.289436
-13.371882	-2.110910	3.681382	0.002415	0.289598
-13.096414	-2.114947	3.691379	0.002364	0.289828
-12.714981	-2.130198	3.701376	0.002293	0.290098
-12.803282	-2.078429	3.711373	0.002309	0.290277
-12.499339	-2.089581	3.721370	0.002253	0.290497
-12.245474	-2.087654	3.731366	0.002205	0.290736
-11.859897	-2.122514	3.741363	0.002134	0.290912
-11.460437	-2.159175	3.751360	0.002059	0.291091
-11.315989	-2.131650	3.761357	0.002032	0.291359
-10.714667	-2.199635	3.771354	0.001920	0.291564
-10.836224	-2.145645	3.781350	0.001943	0.291723
-10.397490	-2.172579	3.791347	0.001861	0.291985
-10.278136	-2.151704	3.801344	0.001839	0.292196
-10.487137	-2.077024	3.811341	0.001877	0.292378
-9.857160	-2.140458	3.821338	0.001760	0.292631
-9.624559	-2.129910	3.831334	0.001717	0.292892
-9.582084	-2.099489	3.841331	0.001709	0.293081
-9.643070	-2.048923	3.851328	0.001720	0.293276
-9.299914	-2.048745	3.861325	0.001656	0.293585
-9.237163	-2.012522	3.871322	0.001644	0.293820
-8.920559	-2.026923	3.881318	0.001585	0.294032
-8.241004	-2.108095	3.891315	0.001459	0.294241
-7.884201	-2.118484	3.901312	0.001392	0.294509
-7.461037	-2.158819	3.911309	0.001314	0.294689
-7.535143	-2.106071	3.921306	0.001327	0.294882
-7.254156	-2.102467	3.931302	0.001275	0.295150
-6.682249	-2.153860	3.941299	0.001168	0.295408
-6.922610	-2.075743	3.951296	0.001213	0.295577
-6.579480	-2.104738	3.961293	0.001149	0.295741
-6.082443	-2.136139	3.971290	0.001056	0.296029
-6.191292	-2.080997	3.981286	0.001077	0.296202
-6.126258	-2.045816	3.991283	0.001064	0.296432
-5.622897	-2.081460	4.001280	0.000971	0.296705
-5.111824	-2.128365	4.011277	0.000876	0.296929
-5.265003	-2.061503	4.021274	0.000904	0.297120
-4.884161	-2.088981	4.031270	0.000833	0.297323
-4.394189	-2.116028	4.041267	0.000742	0.297625
-4.328107	-2.085269	4.051264	0.000729	0.297833
-4.185417	-2.069570	4.061261	0.000703	0.298035
-4.004136	-2.058098	4.071258	0.000669	0.298251
-3.429238	-2.104058	4.081254	0.000562	0.298535
-4.053468	-1.949464	4.091251	0.000678	0.298735
-3.300468	-2.037633	4.101248	0.000538	0.298971
-3.316762	-1.982948	4.111245	0.000541	0.299221
-3.222318	-1.944424	4.121242	0.000523	0.299491
-2.499161	-2.024719	4.131238	0.000388	0.299738
-2.716658	-1.938816	4.141235	0.000429	0.299962
-2.326094	-1.958592	4.151232	0.000356	0.300209
-2.632800	-1.843531	4.161229	0.000413	0.300495
-2.927247	-1.743060	4.171226	0.000468	0.300721
-2.444115	-1.769197	4.181222	0.000378	0.301018
-2.518099	-1.698616	4.191219	0.000391	0.301293
-1.867995	-1.751837	4.201216	0.000270	0.301605
-1.648428	-1.739378	4.211213	0.000229	0.301856
-1.374048	-1.734094	4.221210	0.000178	0.302121
-2.482515	-1.463434	4.231206	0.000384	0.302452
-2.106380	-1.457431	4.241203	0.000314	0.302808
-2.387563	-1.336645	4.251200	0.000366	0.303141
-1.852329	-1.360436	4.261197	0.000267	0.303492
-1.341166	-1.386417	4.271194	0.000171	0.303811
-1.593755	-1.265548	4.281190	0.000218	0.304168
-1.201629	-1.270060	4.291187	0.000145	0.304485
-1.404056	-1.149442	4.301184	0.000183	0.304884
-1.229840	-1.104487	4.311181	0.000150	0.305247
-1.282506	-1.017455	4.321178	0.000160	0.305615
-1.288964	-0.941982	4.331174	0.000161	0.305966
-1.390640	-0.843108	4.341171	0.000180	0.306347
-1.247883	-0.772898	4.351168	0.000153	0.306801
-1.066869	-0.728052	4.361165	0.000119	0.307167
-0.832249	-0.687362	4.371162	0.000076	0.307560
-0.524957	-0.639084	4.381158	0.000018	0.308049
-0.322812	-0.597326	4.391155	-0.000019	0.308418
-0.476601	-0.482583	4.401152	0.000009	0.308825
-1.515971	-0.185431	4.411149	0.000202	0.309332
-1.248386	-0.142374	4.421146	0.000153	0.309761
-1.086017	-0.054348	4.431142	0.000122	0.310310
-0.567125	-0.059577	4.441139	0.000026	0.310725
-0.332227	0.003761	4.451136	-0.000018	0.311218
0.000000	0.026128	4.461133	-0.000080	0.311603

-0.048786	0.314192	4.466138	-0.000071	0.312897
0.039356	0.867182	4.471142	-0.000088	0.315517
-0.100441	1.746074	4.476147	-0.000063	0.319406
0.144181	2.840729	4.481152	-0.000109	0.324525
1.137961	4.095229	4.486157	-0.000295	0.330860
1.563169	5.754929	4.491162	-0.000375	0.338370
1.830845	7.746066	4.496166	-0.000426	0.346981
3.216604	9.842674	4.501171	-0.000686	0.356637
5.483259	12.097507	4.506176	-0.001109	0.367292
6.576148	14.895910	4.511181	-0.001315	0.378910
7.699317	18.032481	4.516186	-0.001526	0.391453
10.141510	21.270927	4.521190	-0.001983	0.404826
12.168069	24.946421	4.526195	-0.002363	0.419020
14.266022	28.965375	4.531200	-0.002756	0.433937
17.867838	33.072325	4.536205	-0.003429	0.449516
21.974896	37.489618	4.541210	-0.004197	0.465818
24.909294	42.485785	4.546214	-0.004746	0.482667
27.958479	47.832406	4.551219	-0.005318	0.500020
31.182852	53.546108	4.556224	-0.005922	0.517901
34.426958	59.576024	4.561229	-0.006530	0.536046
38.272003	65.867330	4.566234	-0.007250	0.554558
42.314905	72.476710	4.571238	-0.008007	0.573360
45.605741	79.557010	4.576243	-0.008624	0.592381
48.912007	86.942378	4.581248	-0.009245	0.611535
55.099224	94.107205	4.586253	-0.010402	0.630782
60.601981	101.727409	4.591258	-0.011431	0.650193
65.010198	109.823929	4.596262	-0.012257	0.669642
69.525539	118.129545	4.601267	-0.013104	0.689017
76.118748	126.307589	4.606272	-0.014337	0.708352
81.022008	135.009628	4.611277	-0.015255	0.727611
84.066206	144.240204	4.616282	-0.015828	0.746751
88.515251	153.346911	4.621286	-0.016663	0.765647
92.027561	162.764310	4.626291	-0.017323	0.784350
95.578868	172.282400	4.631296	-0.017990	0.802807
99.435833	181.822686	4.636301	-0.018715	0.820981
102.837800	191.534574	4.641306	-0.019354	0.838914
107.930668	200.963490	4.646310	-0.020309	0.856495
114.126664	210.288877	4.651315	-0.021469	0.873868
118.709027	219.950995	4.656320	-0.022328	0.890982
123.497771	229.604624	4.661325	-0.023226	0.907815
137.514655	237.727221	4.666330	-0.025841	0.924473
158.229083	244.893971	4.671334	-0.029703	0.941157
172.887918	253.387382	4.676339	-0.032438	0.957937
177.978775	263.596614	4.681344	-0.033393	0.974485
184.774102	273.456021	4.686349	-0.034665	0.990675
194.634605	282.758456	4.691354	-0.036507	1.006566
202.114519	292.479531	4.696358	-0.037906	1.022210
210.411001	302.008481	4.701363	-0.039457	1.037542
220.679702	311.198276	4.706368	-0.041375	1.052648
228.611737	320.776415	4.711373	-0.042858	1.067512
233.813019	330.757636	4.716378	-0.043833	1.082075
237.354682	340.912927	4.721382	-0.044499	1.096294
240.998155	350.880178	4.726387	-0.045184	1.110108
243.910706	360.859299	4.731392	-0.045733	1.123604
247.693734	370.550649	4.736397	-0.046444	1.136763
250.833638	380.266482	4.741402	-0.047035	1.149661
253.066922	389.997452	4.746406	-0.047457	1.162242
255.099673	399.619513	4.751411	-0.047842	1.174511
257.984601	408.995037	4.756416	-0.048385	1.186529
260.819793	418.268925	4.761421	-0.048919	1.198293
263.547568	427.484235	4.766426	-0.049433	1.209850
265.731563	436.709316	4.771430	-0.049846	1.221198
267.920664	445.845007	4.776435	-0.050259	1.232338
269.501115	454.998646	4.781440	-0.050560	1.243278
270.946513	464.085419	4.786445	-0.050835	1.254019
273.167072	472.953406	4.791450	-0.051254	1.264569
275.142697	481.830672	4.796454	-0.051628	1.274994
276.634773	490.709753	4.801459	-0.051911	1.285244
278.319095	499.520767	4.806464	-0.052231	1.295373
279.900565	508.278633	4.811469	-0.052531	1.305344
281.554723	517.069763	4.816474	-0.052845	1.315289
282.875666	525.763285	4.821478	-0.053096	1.324993
284.051626	534.449910	4.826483	-0.053321	1.334591
286.567271	542.864658	4.831488	-0.053795	1.344069
288.734208	551.341808	4.836493	-0.054204	1.353484
290.690425	559.828360	4.841498	-0.054574	1.362806
291.747403	568.466933	4.846502	-0.054776	1.372067
292.929369	577.016820	4.851507	-0.055002	1.381193
294.186457	585.540806	4.856512	-0.055242	1.390246
295.574163	593.984675	4.861517	-0.055505	1.399179
296.708097	602.470162	4.866522	-0.055722	1.408055
298.237717	610.862144	4.871526	-0.056012	1.416846
299.551581	619.250225	4.876531	-0.056263	1.425543
300.464644	627.741214	4.881536	-0.056438	1.434223
302.025822	636.046546	4.886541	-0.056734	1.442772
303.259459	644.436895	4.891546	-0.056969	1.451300
304.446980	652.829202	4.896550	-0.057196	1.459773
306.522567	661.058369	4.901555	-0.057588	1.468180
308.378014	669.368630	4.906560	-0.057939	1.476581
309.905368	677.659612	4.911565	-0.058229	1.484864
311.392404	685.972666	4.916570	-0.058511	1.493115
312.199762	694.379458	4.921574	-0.058667	1.501304
313.615455	702.664027	4.926579	-0.058936	1.509425
315.337092	710.918668	4.931584	-0.059262	1.517522
315.837124	719.346388	4.936589	-0.059361	1.525551
317.409782	727.590342	4.941594	-0.059659	1.533529
319.488513	735.744421	4.946598	-0.060051	1.541457
321.552977	743.925429	4.951603	-0.060441	1.549368
323.730266	752.094672	4.956608	-0.060852	1.557243
324.570318	760.472251	4.961613	-0.061014	1.565070
326.019340	768.748062	4.966618	-0.061289	1.572855
327.071370	777.063593	4.971622	-0.061490	1.580579
328.168640	785.373072	4.976627	-0.061700	1.588266
329.224048	793.666530	4.981632	-0.061902	1.595896
330.688030	801.852249	4.986637	-0.062180	1.603451
331.532347	810.171414	4.991642	-0.062342	1.611000
332.633193	818.424702	4.996646	-0.062553	1.618491
333.943282	826.633802	5.001651	-0.062802	1.625939
335.078079	834.940184	5.006656	-0.063019	1.633413
336.405246	843.082791	5.011661	-0.063271	1.640736
337.608825	851.318372	5.016666	-0.063501	1.648089
338.214024	859.631888	5.021670	-0.063619	1.655395
340.036627	867.692429	5.026675	-0.063964	1.662617
340.998058	875.972074	5.031680	-0.064148	1.669878
341.903591	884.196837	5.036685	-0.064322	1.677052
342.789383	892.417741	5.041690	-0.064492	1.684190
343.622390	900.667246	5.046694	-0.064653	1.691314
344.664152	908.862720	5.051699	-0.064852	1.698391
346.047638	916.992593	5.056704	-0.065115	1.705428
346.922651	925.232015	5.061709	-0.065283	1.712460
348.038056	933.389806	5.066714	-0.065497	1.719427
349.148873	941.556502	5.071718	-0.065709	1.726372
350.171780	949.741864	5.076723	-0.065905	1.733292
351.111824	957.957007	5.081728	-0.066085	1.740199
352.595766	966.045992	5.086733	-0.066367	1.747044
353.311288	974.291443	5.091738	-0.066505	1.753892
353.697887	982.560194	5.096742	-0.066583	1.760690
354.367208	990.757160	5.101747	-0.066713	1.767439
355.629663	998.870676	5.106752	-0.066953	1.774170
356.705031	1006.993106	5.111757	-0.067159	1.780859
357.681631	1015.175189	5.116762	-0.067346	1.787557
359.330240	1023.268935	5.121766	-0.067658	1.794244
360.268475	1031.409290	5.126771	-0.067838	1.800854
360.729320	1039.685769	5.131776	-0.067929	1.807489
360.988877	1047.948860	5.136781	-0.067983	1.814064
361.729355	1056.077708	5.141786	-0.068126	1.820569
362.753806	1064.181195	5.146790	-0.068322	1.827064
363.332508	1072.393029	5.151795	-0.068435	1.833567
363.704596	1080.593494	5.156800	-0.068510	1.840014
364.152337	1088.766239	5.161805	-0.068599	1.846425
365.208168	1096.856711	5.166810	-0.068801	1.852822
366.320046	1104.952183	5.171814	-0.069013	1.859208
367.136315	1113.081204	5.176819	-0.069170	1.865562
368.623080	1121.127404	5.181824	-0.069452	1.871910
369.973626	1129.184882	5.186829	-0.069709	1.878228
371.242010	1137.273447	5.191834	-0.069951	1.884539
372.410782	1145.408787	5.196838	-0.070174	1.890853
373.744802	1153.494799	5.201843	-0.070427	1.897127
374.852767	1161.652910	5.206848	-0.070639	1.903408
375.480255	1169.863043	5.211853	-0.070761	1.909652
376.596229	1177.978418	5.216858	-0.070974	1.915861
377.457677	1186.148572	5.221862	-0.071140	1.922061
378.917466	1194.207378	5.226867	-0.071417	1.928225
380.929142	1202.223267	5.231872	-0.071797	1.934399
381.881690	1210.383534	5.236877	-0.071980	1.940542
382.303816	1218.651646	5.241882	-0.072064	1.946686
383.466206	1226.746717	5.246886	-0.072285	1.952765
384.697526	1234.810975	5.251891	-0.072520	1.958809
385.692834	1242.940259	5.256896	-0.072711	1.964857
386.435993	1251.096517	5.261901	-0.072854	1.970877
387.431672	1259.232005	5.266906	-0.073045	1.976892
388.929551	1267.276466	5.271910	-0.073329	1.982876
389.680401	1275.443418	5.276915	-0.073474	1.988850
390.696862	1283.584514	5.281920	-0.073669	1.994815
392.656304	1291.538691	5.286925	-0.074039	2.000729
393.771414	1299.676275	5.291930	-0.074252	2.006667
394.985848	1307.819588	5.296934	-0.074484	2.012601
396.200943	1315.931143	5.301939	-0.074715	2.018495
398.145315	1323.962002	5.306944	-0.075082	2.024390
400.312452	1331.948071	5.311949	-0.075491	2.030260
401.700061	1340.067630	5.316954	-0.075755	2.036125
402.873150	1348.197091	5.321958	-0.075979	2.041957
402.958439	1356.511698	5.326963	-0.076000	2.047790
404.258680	1364.607843	5.331968	-0.076247	2.053579
405.026177	1372.764102	5.336973	-0.076396	2.059339
406.321857	1380.831351	5.341978	-0.076642	2.065074
407.052215	1389.022180	5.346982	-0.076783	2.070821
408.156239	1397.093293	5.351987	-0.076994	2.076507
409.061477	1405.222563	5.356992	-0.077168	2.082197
409.882955	1413.345602	5.361997	-0.077326	2.087859
410.737860	1421.461401	5.367002	-0.077491	2.093504
411.517335	1429.593831	5.372006	-0.077641	2.099137
412.726941	1437.604428	5.377011	-0.077872	2.104715
413.654753	1445.758814	5.382016	-0.078050	2.110347
414.713362	1453.863761	5.387021	-0.078252	2.115943
415.585258	1461.930806	5.392026	-0.078420	2.121481
416.606402	1470.013855	5.397030	-0.078616	2.127029
417.790224	1478.078175	5.402035	-0.078841	2.132565
418.979866	1486.149100	5.407040	-0.079068	2.138092
419.583546	1494.305011	5.412045	-0.079186	2.143605
420.779297	1502.366985	5.417050	-0.079414	2.149098
421.534026	1510.496094	5.422054	-0.079560	2.154578
422.865850	1518.505986	5.427059	-0.079813	2.160021
424.301168	1526.542864	5.432064	-0.080085	2.165477
425.565037	1534.604044	5.437069	-0.080326	2.170919
426.081542	1542.808817	5.442074	-0.080427	2.176371
426.971815	1550.924533	5.447078	-0.080599	2.181786
427.754565	1559.034400	5.452083	-0.080750	2.187173
429.037936	1567.115356	5.457088	-0.080994	2.192575
429.909330	1575.213271	5.462093	-0.081161	2.197936
431.301767	1583.203602	5.467098	-0.081426	2.203262
432.555142	1591.269128	5.472102	-0.081665	2.208610
433.609960	1599.357089	5.477107	-0.081866	2.213942
434.261738	1607.521157	5.482112	-0.081993	2.219273
435.119229	1615.594407	5.487117	-0.082158	2.224551
435.651449	1623.785215	5.492122	-0.082262	2.229862
436.686846	1631.830542	5.497126	-0.082460	2.235113
437.296225	1639.930066	5.502131	-0.082579	2.240348
438.671445	1647.951661	5.507136	-0.082841	2.245589
439.611444	1656.044719	5.512141	-0.083021	2.250824
440.146978	1664.194291	5.517146	-0.083126	2.256047
441.597586	1672.196478	5.522150	-0.083401	2.261246
442.793167	1680.232345	5.527155	-0.083629	2.266430
444.387994	1688.302667	5.532160	-0.083931	2.271659
445.821493	1696.320241	5.537165	-0.084204	2.276829
447.107988	1704.361748	5.542170	-0.084448	2.281989
448.392694	1712.450085	5.547174	-0.084693	2.287166
448.953331	1720.628394	5.552179	-0.084803	2.292324
449.845318	1728.718692	5.557184	-0.084974	2.297445
450.563337	1736.812191	5.562189	-0.085113	2.302541
451.662111	1744.849135	5.567194	-0.085323	2.307623
452.632000	1752.957603	5.572198	-0.085509	2.312727
453.626265	1761.018110	5.577203	-0.085699	2.317792
455.007058	1769.034166	5.582208	-0.085962	2.322850
455.915399	1777.137564	5.587213	-0.086136	2.327912
457.058425	1785.211178	5.592218	-0.086354	2.332963
457.767627	1793.338490	5.597222	-0.086492	2.338000
459.411902	1801.270684	5.602227	-0.086803	2.342985
460.329536	1809.428806	5.607232	-0.086979	2.348036
461.529701	1817.479759	5.612237	-0.087208	2.353034
462.962632	1825.509674	5.617242	-0.087480	2.358028
463.894087	1833.611257	5.622246	-0.087659	2.363013
464.608446	1841.717534	5.627251	-0.087797	2.367972
465.289126	1849.865014	5.632256	-0.087929	2.372943
465.821554	1857.944125	5.637261	-0.088034	2.377851
465.982653	1866.111295	5.642266	-0.088069	2.382771
466.694110	1874.193163	5.647270	-0.088207	2.387674
467.059541	1882.289689	5.652275	-0.088280	2.392547
468.105204	1890.276326	5.657280	-0.088480	2.397400
468.937028	1898.310012	5.662285	-0.088640	2.402253
469.056607	1906.468191	5.667290	-0.088668	2.407114
469.360916	1914.602534	5.672294	-0.088730	2.411966
469.848902	1922.654364	5.677299	-0.088826	2.416773
470.707747	1930.692577	5.682304	-0.088991	2.421592
470.859297	1938.803614	5.687309	-0.089025	2.426389
471.559014	1946.886320	5.692314	-0.089160	2.431202
472.034569	1954.972090	5.697318	-0.089254	2.435990
472.618686	1962.968621	5.702323	-0.089368	2.440724
473.247641	1970.999451	5.707328	-0.089490	2.445473
473.711745	1979.092899	5.712333	-0.089582	2.450236
474.174704	1987.139575	5.717338	-0.089674	2.454963
474.720132	1995.201983	5.722342	-0.089780	2.459696
475.704560	2003.168649	5.727347	-0.089969	2.464397
477.002593	2011.162151	5.732352	-0.090216	2.469129
477.115180	2019.372160	5.737357	-0.090242	2.473886
477.762040	2027.406821	5.742362	-0.090368	2.478574
478.995058	2035.382909	5.747366	-0.090603	2.483263
479.554798	2043.458127	5.752371	-0.090712	2.487949
480.215363	2051.574220	5.757376	-0.090841	2.492658
480.717558	2059.638283	5.762381	-0.090939	2.497316
480.961763	2067.759069	5.767386	-0.090990	2.501978
481.748843	2075.792122	5.772390	-0.091142	2.506622
482.559459	2083.807103	5.777395	-0.091298	2.511248
482.910909	2091.916089	5.782400	-0.091369	2.515886
482.976046	2100.030058	5.787405	-0.091386	2.520496
483.721896	2108.016574	5.792410	-0.091530	2.525076
484.248041	2116.109247	5.797414	-0.091634	2.529691
484.378981	2124.180222	5.802419	-0.091663	2.534257
484.971552	2132.231740	5.807424	-0.091779	2.538837
485.601307	2140.243431	5.812429	-0.091901	2.543389
485.748595	2148.374262	5.817434	-0.091934	2.547965
486.335103	2156.436562	5.822438	-0.092049	2.552526
487.379984	2164.361826	5.827443	-0.092248	2.557034
487.745463	2172.474704	5.832448	-0.092322	2.561591
488.273361	2180.515537	5.837453	-0.092425	2.566111
488.981097	2188.552898	5.842458	-0.092562	2.570633
490.032163	2196.567669	5.847462	-0.092763	2.575159
490.715451	2204.598796	5.852467	-0.092896	2.579660
491.191803	2212.711089	5.857472	-0.092990	2.584184
490.981445	2220.913230	5.862477	-0.092956	2.588701
491.299644	2229.045937	5.867482	-0.093021	2.593209
491.872632	2237.048702	5.872486	-0.093133	2.597656
492.831167	2244.958160	5.877491	-0.093316	2.602069
493.472648	2253.017776	5.882496	-0.093441	2.606536
493.609397	2261.136052	5.887501	-0.093472	2.610992
494.223016	2269.146892	5.892506	-0.093591	2.615415
494.474358	2277.249641	5.897510	-0.093643	2.619856
494.639350	2285.292454	5.902515	-0.093679	2.624250
494.687190	2293.423108	5.907520	-0.093694	2.628677
495.389040	2301.405728	5.912525	-0.093830	2.633060
496.104643	2309.396057	5.917530	-0.093968	2.637441
496.964593	2317.372775	5.922534	-0.094133	2.641817
497.282055	2325.446837	5.927539	-0.094198	2.646201
497.880353	2333.523983	5.932544	-0.094314	2.650599
498.180725	2341.645404	5.937549	-0.094376	2.654993
498.939896	2349.628058	5.942554	-0.094522	2.659336
499.851678	2357.631732	5.947558	-0.094697	2.663693
500.051608	2365.752374	5.952563	-0.094740	2.668058
500.764173	2373.802295	5.957568	-0.094878	2.672412
501.500306	2381.810266	5.962573	-0.095020	2.676738
501.762915	2389.897422	5.967578	-0.095074	2.681068
502.094007	2397.939624	5.972582	-0.095141	2.685372
502.124505	2406.054876	5.977587	-0.095152	2.689688
502.877487	2414.069268	5.982592	-0.095298	2.693990
503.057660	2422.146080	5.987597	-0.095337	2.698282
503.093451	2430.231430	5.992602	-0.095348	2.702562
503.787185	2438.242112	5.997606	-0.095483	2.706837
504.154129	2446.295684	6.002611	-0.095557	2.711108
504.249333	2454.397168	6.007616	-0.095580	2.715380
505.527274	2462.262762	6.012621	-0.095823	2.719596
506.139380	2470.287041	6.017626	-0.095942	2.723846
506.339238	2478.443212	6.022630	-0.095984	2.728133
506.720638	2486.483206	6.027635	-0.096061	2.732363
507.391621	2494.512180	6.032640	-0.096191	2.736600
507.491810	2502.626623	6.037645	-0.096215	2.740838
507.842383	2510.641795	6.042650	-0.096285	2.745034
508.553964	2518.658522	6.047654	-0.096423	2.749247
508.339640	2526.855831	6.052659	-0.096389	2.753490
508.582291	2534.911668	6.057664	-0.096439	2.757681
508.899738	2542.914955	6.062669	-0.096503	2.761842
509.274510	2550.902600	6.067674	-0.096578	2.765993
508.888312	2559.088730	6.072678	-0.096512	2.770194
509.062660	2567.093392	6.077683	-0.096550	2.774330
509.626157	2575.097941	6.082688	-0.096660	2.778482
510.423696	2583.032091	6.087693	-0.096813	2.782606
510.970187	2591.060147	6.092698	-0.096920	2.786756
511.244613	2599.169394	6.097702	-0.096977	2.790926
511.868261	2607.159293	6.102707	-0.097098	2.795049
512.417561	2615.178548	6.107712	-0.097206	2.799177
512.979834	2623.203552	6.112717	-0.097316	2.803302
513.396926	2631.271001	6.117722	-0.097399	2.807434
514.158172	2639.319432	6.122726	-0.097546	2.811570
514.714262	2647.344723	6.127731	-0.097655	2.815677
515.578015	2655.342939	6.132736	-0.097821	2.819781
516.242901	2663.377388	6.137741	-0.097950	2.823886
516.924019	2671.414630	6.142746	-0.098082	2.827988
517.188049	2679.545126	6.147750	-0.098136	2.832106
517.615154	2687.580928	6.152755	-0.098221	2.836180
518.195711	2695.591771	6.157760	-0.098334	2.840244
518.260329	2703.674440	6.162765	-0.098352	2.844309
518.965771	2711.678401	6.167770	-0.098488	2.848365
519.598933	2719.764738	6.172774	-0.098611	2.852452
519.662165	2727.853934	6.177779	-0.098629	2.856503
520.496237	2735.829299	6.182784	-0.098789	2.860534
520.547608	2743.924194	6.187789	-0.098804	2.864575
520.981021	2751.954246	6.192794	-0.098890	2.868600
521.992615	2759.928868	6.197798	-0.099084	2.872624
522.142426	2768.012683	6.202803	-0.099117	2.876648
522.792251	2776.053722	6.207808	-0.099243	2.880672
523.174993	2784.084554	6.212813	-0.099319	2.884672
523.541673	2792.138650	6.217818	-0.099393	2.888676
524.201708	2800.196704	6.222822	-0.099521	2.892693
524.644778	2808.222087	6.227827	-0.099609	2.896676
525.042996	2816.292293	6.232832	-0.099688	2.900673
525.937085	2824.231187	6.237837	-0.099860	2.904627
526.289943	2832.327202	6.242842	-0.099931	2.908623
526.989563	2840.407676	6.247846	-0.100067	2.912625
526.995108	2848.526514	6.252851	-0.100073	2.916602
527.066750	2856.608290	6.257856	-0.100092	2.920560
527.679060	2864.544413	6.262861	-0.100211	2.924470
528.199234	2872.546432	6.267866	-0.100313	2.928402
529.127126	2880.528281	6.272870	-0.100491	2.932340
529.301490	2888.617923	6.277875	-0.100529	2.936285
529.892464	2896.646696	6.282880	-0.100644	2.940218
530.123015	2904.701362	6.287885	-0.100692	2.944138
530.627469	2912.733874	6.292890	-0.100791	2.948057
531.301391	2920.761533	6.297894	-0.100922	2.951978
531.614312	2928.800581	6.302899	-0.100986	2.955879
532.213734	2936.811011	6.307904	-0.101103	2.959777
532.928002	2944.793350	6.312909	-0.101241	2.963662
533.221313	2952.866332	6.317914	-0.101301	2.967563
533.364192	2960.999434	6.322918	-0.101333	2.971480
533.970408	2968.984913	6.327923	-0.101451	2.975345
534.140290	2977.082620	6.332928	-0.101488	2.979236
534.749738	2985.072856	6.337933	-0.101606	2.983094
535.149968	2993.092194	6.342938	-0.101686	2.986949
535.722708	3001.150817	6.347942	-0.101798	2.990827
536.209179	3009.156690	6.352947	-0.101894	2.994670
536.502166	3017.202191	6.357952	-0.101954	2.998517
536.948111	3025.244596	6.362957	-0.102042	3.002366
536.182741	3033.469165	6.367962	-0.101905	3.006235
537.168698	3041.358275	6.372966	-0.102094	3.010028
537.374191	3049.416626	6.377971	-0.102137	3.013857
538.002846	3057.413080	6.382976	-0.102260	3.017673
538.043510	3065.498288	6.387981	-0.102272	3.021497
538.419452	3073.495746	6.392986	-0.102348	3.025291
538.837842	3081.551348	6.397990	-0.102431	3.029110
539.165681	3089.594959	6.402995	-0.102497	3.032913
539.558082	3097.635473	6.408000	-0.102575	3.036714
540.231844	3105.619082	6.413005	-0.102706	3.040497
540.492598	3113.622599	6.418010	-0.102760	3.044264
540.799477	3121.756073	6.423014	-0.102822	3.048090
540.366089	3129.891752	6.428019	-0.102747	3.051876
540.850226	3137.890414	6.433024	-0.102842	3.055638
541.484989	3145.833470	6.438029	-0.102966	3.059376
541.891095	3153.850978	6.443034	-0.103047	3.063134
542.210710	3161.938420	6.448038	-0.103111	3.066915
542.183104	3170.052796	6.453043	-0.103112	3.070687
543.122184	3178.011668	6.458048	-0.103292	3.074428
543.091300	3186.059564	6.463053	-0.103291	3.078160
543.185117	3194.093049	6.468058	-0.103314	3.081887
543.912606	3202.040808	6.473062	-0.103455	3.085599
544.233365	3210.056031	6.478067	-0.103520	3.089319
544.451412	3218.150364	6.483072	-0.103566	3.093066
544.686204	3226.236003	6.488077	-0.103615	3.096806
545.571873	3234.140363	6.493082	-0.103785	3.100487
545.882154	3242.170263	6.498086	-0.103848	3.104195
545.828623	3250.296142	6.503091	-0.103843	3.107926
546.505734	3258.295824	6.508096	-0.103974	3.111628
546.918632	3266.348886	6.513101	-0.104057	3.115338
546.623509	3274.412242	6.518106	-0.104007	3.119016
547.509428	3282.365114	6.523110	-0.104177	3.122692
547.758331	3290.415859	6.528115	-0.104229	3.126380
547.638663	3298.530671	6.533120	-0.104212	3.130076
547.737748	3306.586020	6.538125	-0.104235	3.133751
548.446869	3314.512255	6.543130	-0.104373	3.137390
548.321553	3322.668612	6.548134	-0.104355	3.141092
548.088684	3330.730230	6.553139	-0.104317	3.144741
549.016024	3338.644945	6.558144	-0.104494	3.148372
549.462664	3346.683363	6.563149	-0.104583	3.152033
549.868062	3354.693283	6.568154	-0.104664	3.155675
549.945122	3362.784178	6.573158	-0.104683	3.159334
550.181500	3370.790748	6.578163	-0.104732	3.162959
551.327648	3378.720793	6.583168	-0.104951	3.166584
552.119617	3386.749045	6.588173	-0.105104	3.170234
552.757867	3394.788674	6.593178	-0.105228	3.173878
552.908772	3402.919117	6.598182	-0.105261	3.177537
553.048119	3410.953627	6.603187	-0.105293	3.181149
553.742648	3418.931975	6.608192	-0.105427	3.184755
553.788785	3427.025360	6.613197	-0.105441	3.188381
553.820928	3435.104884	6.618202	-0.105452	3.191995
554.327056	3443.123000	6.623206	-0.105552	3.195599
554.313820	3451.173485	6.628211	-0.105555	3.199190
554.231809	3459.217853	6.633216	-0.105545	3.202772
554.724416	3467.222086	6.638221	-0.105642	3.206357
555.171236	3475.208972	6.643226	-0.105730	3.209927
555.643110	3483.253237	6.648230	-0.105823	3.213520
555.555753	3491.327993	6.653235	-0.105812	3.217099
556.044750	3499.330489	6.658240	-0.105908	3.220667
555.982353	3507.399719	6.663245	-0.105902	3.224236
556.023729	3515.446210	6.668250	-0.105915	3.227796
556.549425	3523.472421	6.673254	-0.106018	3.231364
557.065206	3531.412416	6.678259	-0.106119	3.234888
557.552900	3539.383093	6.683264	-0.106215	3.238422
557.692182	3547.481069	6.688269	-0.106247	3.241992
557.742211	3555.525327	6.693274	-0.106261	3.245532
558.193610	3563.551076	6.698278	-0.106351	3.249076
558.441159	3571.584779	6.703283	-0.106402	3.252612
558.720677	3579.616556	6.708288	-0.106459	3.256144
559.180419	3587.624159	6.713293	-0.106550	3.259668
559.412927	3595.628734	6.718298	-0.106599	3.263179
560.284567	3603.619067	6.723302	-0.106766	3.266705
560.340963	3611.715412	6.728307	-0.106782	3.270240
560.699284	3619.717693	6.733312	-0.106854	3.273743
561.168190	3627.756648	6.738317	-0.106947	3.277263
560.530806	3635.896656	6.743322	-0.106833	3.280778
561.142076	3643.830216	6.748326	-0.106952	3.284250
561.158780	3651.889738	6.753331	-0.106961	3.287749
561.516020	3659.931358	6.758336	-0.107032	3.291250
561.714091	3667.969417	6.763341	-0.107075	3.294740
562.082920	3675.978331	6.768346	-0.107148	3.298219
562.396812	3684.009503	6.773350	-0.107212	3.301703
562.417350	3692.066236	6.778355	-0.107221	3.305182
562.862573	3700.075345	6.783360	-0.107309	3.308654
562.809469	3708.184011	6.788365	-0.107305	3.312146
562.708813	3716.240863	6.793370	-0.107291	3.315610
563.315443	3724.153096	6.798374	-0.107410	3.319035
563.567680	3732.149620	6.803379	-0.107462	3.322479
563.931877	3740.179600	6.808384	-0.107535	3.325938
564.657433	3748.155583	6.813389	-0.107675	3.329384
564.374377	3756.274348	6.818394	-0.107628	3.332850
564.609313	3764.363897	6.823398	-0.107677	3.336318
564.733586	3772.348881	6.828403	-0.107705	3.339735
565.018845	3780.371918	6.833408	-0.107764	3.343170
565.377734	3788.406440	6.838413	-0.107836	3.346609
565.262291	3796.466564	6.843418	-0.107819	3.350038
566.072647	3804.391227	6.848422	-0.107975	3.353440
566.133344	3812.456272	6.853427	-0.107992	3.356871
566.614940	3820.477706	6.858432	-0.108087	3.360295
567.065611	3828.471941	6.863437	-0.108176	3.363702
567.110436	3836.536029	6.868442	-0.108190	3.367121
567.577575	3844.600795	6.873446	-0.108282	3.370552
567.602367	3852.624814	6.878451	-0.108292	3.373946
567.890327	3860.669889	6.883456	-0.108351	3.377356
568.404680	3868.673554	6.888461	-0.108452	3.380752
568.953435	3876.593684	6.893466	-0.108559	3.384111
569.018972	3884.743252	6.898470	-0.108577	3.387546
569.107483	3892.810838	6.903475	-0.108599	3.390944
569.784875	3900.789909	6.908480	-0.108730	3.394322
569.730994	3908.881407	6.913485	-0.108725	3.397717
570.017750	3916.851019	6.918490	-0.108784	3.401071
570.194688	3924.863955	6.923494	-0.108822	3.404435
570.342450	3932.889594	6.928499	-0.108855	3.407800
570.536783	3940.947726	6.933504	-0.108896	3.411177
570.943301	3948.937176	6.938509	-0.108977	3.414530
571.184098	3956.968680	6.943514	-0.109027	3.417890
571.700999	3964.992765	6.948518	-0.109129	3.421254
571.366381	3973.052831	6.953523	-0.109072	3.424601
571.539363	3981.088418	6.958528	-0.109109	3.427951
571.874833	3989.152359	6.963533	-0.109177	3.431315
572.081768	3997.098093	6.968538	-0.109221	3.434623
572.557766	4005.101763	6.973542	-0.109315	3.437960
572.855309	4013.148401	6.978547	-0.109375	3.441306
572.884516	4021.168375	6.983552	-0.109386	3.444628
573.495007	4029.160060	6.988557	-0.109505	3.447955
574.145532	4037.150458	6.993562	-0.109631	3.451280
574.394307	4045.223064	6.998566	-0.109683	3.454622
574.333120	4053.305976	7.003571	-0.109677	3.457954
574.526736	4061.359423	7.008576	-0.109718	3.461280
575.306157	4069.290096	7.013581	-0.109868	3.464571
575.842831	4077.308929	7.018586	-0.109974	3.467887
576.465325	4085.344023	7.023590	-0.110095	3.471210
576.422795	4093.425813	7.028595	-0.110092	3.474526
577.219464	4101.383669	7.033600	-0.110246	3.477816
577.102181	4109.520467	7.038605	-0.110229	3.481146
577.440975	4117.457908	7.043610	-0.110297	3.484407
577.473481	4125.568480	7.048614	-0.110309	3.487725
577.948335	4133.584603	7.053619	-0.110402	3.491015
578.197742	4141.566587	7.058624	-0.110454	3.494282
578.625499	4149.595766	7.063629	-0.110539	3.497570
578.368939	4157.719294	7.068634	-0.110497	3.500871
578.446476	4165.703790	7.073638	-0.110516	3.504124
578.929802	4173.724786	7.078643	-0.110611	3.507401
578.873070	4181.837032	7.083648	-0.110606	3.510695
579.875582	4189.696947	7.088653	-0.110798	3.513917
580.014374	4197.755388	7.093658	-0.110829	3.517189
579.817926	4205.860386	7.098662	-0.110798	3.520466
579.866745	4213.845936	7.103667	-0.110812	3.523700
580.311949	4221.845486	7.108672	-0.110900	3.526949
580.518052	4229.894133	7.113677	-0.110944	3.530207
580.582070	4237.938732	7.118682	-0.110961	3.533456
581.028573	4245.956203	7.123686	-0.111050	3.536703
581.506953	4253.908284	7.128691	-0.111144	3.539921
581.727735	4261.969611	7.133696	-0.111190	3.543173
582.097992	4269.989869	7.138701	-0.111264	3.546410
582.477595	4278.004488	7.143706	-0.111340	3.549641
582.824587	4286.114640	7.148710	-0.111410	3.552907
583.075510	4294.142274	7.153715	-0.111462	3.556134
583.767158	4302.015717	7.158720	-0.111596	3.559309
584.123902	4310.093946	7.163725	-0.111668	3.562554
584.487801	4318.104204	7.168730	-0.111741	3.565768
585.038145	4326.094734	7.173734	-0.111849	3.568977
585.309008	4334.143923	7.178739	-0.111904	3.572199
585.433142	4342.243453	7.183744	-0.111933	3.575433
585.447968	4350.270642	7.188749	-0.111941	3.578632
585.708979	4358.260270	7.193754	-0.111995	3.581820
586.199484	4366.251324	7.198758	-0.112091	3.585013
586.076086	4374.353532	7.203763	-0.112074	3.588229
585.972844	4382.460706	7.208768	-0.112060	3.591445
585.992622	4390.465385	7.213773	-0.112069	3.594621
586.523280	4398.406247	7.218778	-0.112173	3.597784
586.745048	4406.470532	7.223782	-0.112219	3.600984
586.969290	4414.411660	7.228787	-0.112266	3.604132
587.488488	4422.438195	7.233792	-0.112368	3.607320
588.012195	4430.478868	7.238797	-0.112471	3.610510
588.029927	4438.529036	7.243802	-0.112479	3.613687
588.278344	4446.599171	7.248806	-0.112531	3.616875
588.709948	4454.546955	7.253811	-0.112617	3.620018
588.538564	4462.616827	7.258816	-0.112590	3.623189
588.748664	4470.676256	7.263821	-0.112634	3.626364
589.310593	4478.605142	7.268826	-0.112744	3.629494
589.787176	4486.651380	7.273830	-0.112838	3.632666
589.935103	4494.689688	7.278835	-0.112871	3.635822
590.315578	4502.664588	7.283840	-0.112947	3.638957
590.632186	4510.713231	7.288845	-0.113011	3.642116
590.948034	4518.679628	7.293850	-0.113075	3.645241
590.916180	4526.809791	7.298854	-0.113075	3.648417
591.623939	4534.780705	7.303859	-0.113212	3.651549
591.698742	4542.812834	7.308864	-0.113231	3.654684
591.854979	4550.871945	7.313869	-0.113265	3.657830
592.140733	4558.888290	7.318874	-0.113324	3.660959
592.857968	4566.831565	7.323878	-0.113462	3.664069
592.856733	4574.926493	7.328883	-0.113468	3.667216
592.994499	4582.963451	7.333888	-0.113498	3.670341
593.569690	4590.965615	7.338893	-0.113611	3.673462
593.593368	4598.993589	7.343898	-0.113620	3.676576
594.084720	4607.026705	7.348902	-0.113717	3.679701
594.342908	4615.044620	7.353907	-0.113771	3.682811
594.240496	4623.124276	7.358912	-0.113757	3.685933
594.257833	4631.152637	7.363917	-0.113765	3.689036
594.193841	4639.183481	7.368922	-0.113759	3.692136
594.515733	4647.204336	7.373926	-0.113824	3.695238
595.238541	4655.112362	7.378931	-0.113964	3.698305
595.214869	4663.210358	7.383936	-0.113964	3.701423
595.558096	4671.198509	7.388941	-0.114034	3.704506
595.662719	4679.258680	7.393946	-0.114058	3.707608
596.421532	4687.238958	7.398950	-0.114205	3.710693
596.613079	4695.344590	7.403955	-0.114246	3.713809
596.803387	4703.370064	7.408960	-0.114287	3.716891
596.811197	4711.380705	7.413965	-0.114293	3.719961
597.148552	4719.295102	7.418970	-0.114361	3.723000
597.214733	4727.395243	7.423974	-0.114379	3.726100
597.605180	4735.350602	7.428979	-0.114457	3.729151
597.881671	4743.423810	7.433984	-0.114514	3.732241
598.590846	4751.409102	7.438989	-0.114651	3.735305
599.244265	4759.351578	7.443994	-0.114778	3.738350
599.217419	4767.503035	7.448998	-0.114778	3.741455
599.357995	4775.485747	7.454003	-0.114809	3.744497
599.530834	4783.517329	7.459008	-0.114847	3.747556
599.626434	4791.625338	7.464013	-0.114870	3.750639
599.589254	4799.630770	7.469018	-0.114868	3.753678
600.369577	4807.603133	7.474022	-0.115019	3.756721
600.649556	4815.578047	7.479027	-0.115076	3.759751
600.688078	4823.631406	7.484032	-0.115089	3.762803
601.072860	4831.678152	7.489037	-0.115166	3.765857
601.340281	4839.633135	7.494042	-0.115221	3.768872
601.634404	4847.743403	7.499046	-0.115281	3.771943
602.082781	4855.674764	7.504051	-0.115369	3.774948
602.542657	4863.703842	7.509056	-0.115460	3.777988
602.444875	4871.868017	7.514061	-0.115447	3.781063
602.356797	4879.834219	7.519066	-0.115436	3.784061
602.764915	4887.875441	7.524070	-0.115517	3.787097
602.961117	4895.878774	7.529075	-0.115559	3.790111
603.445329	4903.886218	7.534080	-0.115655	3.793131
604.058367	4911.928317	7.539085	-0.115774	3.796164
604.720623	4919.801007	7.544090	-0.115903	3.799132
605.113244	4927.883682	7.549094	-0.115981	3.802170
604.615930	4935.974933	7.554099	-0.115894	3.805189
605.194241	4943.968733	7.559104	-0.116007	3.808194
605.986963	4951.976516	7.564109	-0.116159	3.811205
605.866461	4959.985281	7.569114	-0.116142	3.814195
606.353588	4968.087690	7.574118	-0.116238	3.817231
606.389938	4976.058131	7.579123	-0.116250	3.820205
606.534398	4984.083821	7.584128	-0.116282	3.823199
607.253129	4992.123683	7.589133	-0.116421	3.826209
607.390899	5000.114793	7.594138	-0.116452	3.829186
608.012820	5008.148993	7.599142	-0.116573	3.832187
608.085037	5016.201130	7.604147	-0.116592	3.835180
608.078692	5024.259041	7.609152	-0.116596	3.838172
608.349996	5032.287219	7.614157	-0.116652	3.841156
608.747305	5040.183174	7.619162	-0.116731	3.844091
609.448110	5048.194649	7.624166	-0.116867	3.847073
609.773537	5056.268420	7.629171	-0.116933	3.850068
609.976925	5064.284543	7.634176	-0.116976	3.853037
610.554447	5072.339243	7.639181	-0.117089	3.856025
610.823951	5080.312751	7.644186	-0.117144	3.858975
611.629538	5088.312623	7.649190	-0.117299	3.861943
611.877871	5096.361739	7.654195	-0.117351	3.864915
612.506168	5104.370758	7.659200	-0.117473	3.867878
612.163701	5112.562628	7.664205	-0.117415	3.870887
612.263394	5120.654127	7.669210	-0.117439	3.873865
612.636436	5128.612053	7.674214	-0.117513	3.876797
613.071133	5136.529444	7.679219	-0.117599	3.879713
613.446742	5144.487680	7.684224	-0.117675	3.882641
613.930381	5152.464142	7.689229	-0.117770	3.885576
613.832668	5160.533551	7.694234	-0.117757	3.888530
614.321420	5168.546045	7.699238	-0.117853	3.891473
614.160435	5176.668694	7.704243	-0.117829	3.894442
614.656314	5184.606158	7.709248	-0.117926	3.897353
614.994071	5192.615451	7.714253	-0.117994	3.900285
615.136923	5200.621543	7.719258	-0.118026	3.903210
615.348367	5208.731144	7.724262	-0.118071	3.906172
615.495406	5216.723546	7.729267	-0.118103	3.909088
615.674533	5224.770050	7.734272	-0.118142	3.912021
616.004932	5232.785622	7.739277	-0.118209	3.914945
616.514596	5240.721595	7.744282	-0.118309	3.917840
616.862160	5248.788079	7.749286	-0.118379	3.920777
617.278680	5256.764318	7.754291	-0.118462	3.923681
617.357910	5264.819042	7.759296	-0.118482	3.926605
617.781384	5272.844135	7.764301	-0.118566	3.929522
617.843281	5280.880848	7.769306	-0.118583	3.932435
618.406619	5288.916254	7.774310	-0.118693	3.935354
618.417295	5296.931385	7.779315	-0.118700	3.938253
618.246056	5305.019476	7.784320	-0.118673	3.941173
618.017014	5313.050680	7.789325	-0.118636	3.944070
618.491250	5321.018850	7.794330	-0.118729	3.946954
618.473936	5329.066855	7.799334	-0.118732	3.949857
618.915250	5337.040006	7.804339	-0.118819	3.952738
619.195746	5345.061793	7.809344	-0.118876	3.955632
619.950850	5353.008986	7.814349	-0.119022	3.958505
619.642795	5361.084651	7.819354	-0.118970	3.961403
620.372139	5369.011251	7.824358	-0.119111	3.964264
620.424605	5377.137663	7.829363	-0.119126	3.967183
620.493148	5385.131781	7.834368	-0.119144	3.970053
621.087868	5393.183044	7.839373	-0.119260	3.972950
620.885367	5401.235953	7.844378	-0.119228	3.975831
621.100511	5409.171744	7.849382	-0.119273	3.978676
621.378881	5417.216811	7.854387	-0.119330	3.981559
621.668749	5425.195652	7.859392	-0.119389	3.984416
621.891398	5433.307668	7.864397	-0.119436	3.987318
621.878124	5441.294166	7.869402	-0.119439	3.990168
622.330997	5449.288213	7.874406	-0.119528	3.993027
622.466413	5457.338023	7.879411	-0.119559	3.995899
622.563157	5465.328845	7.884416	-0.119582	3.998747
622.708329	5473.390737	7.889421	-0.119615	4.001619
623.099206	5481.312846	7.894426	-0.119692	4.004443
623.531280	5489.381182	7.899430	-0.119778	4.007318
623.604022	5497.433197	7.904435	-0.119797	4.010179
624.000396	5505.416470	7.909440	-0.119876	4.013019
624.631124	5513.449577	7.914445	-0.119999	4.015878
624.882274	5521.442318	7.919450	-0.120051	4.018714
625.296646	5529.463490	7.924454	-0.120133	4.021562
626.068617	5537.426922	7.929459	-0.120282	4.024392
626.307803	5545.484426	7.934464	-0.120332	4.027245
626.561889	5553.596586	7.939469	-0.120385	4.030116
626.722197	5561.660403	7.944474	-0.120420	4.032966
626.946456	5569.686486	7.949478	-0.120467	4.035802
627.282537	5577.650555	7.954483	-0.120535	4.038615
628.045865	5585.613293	7.959488	-0.120682	4.041433
628.508083	5593.586954	7.964493	-0.120773	4.044248
628.270956	5601.697648	7.969498	-0.120734	4.047098
628.578999	5609.708013	7.974502	-0.120797	4.049919
629.332483	5617.713995	7.979507	-0.120943	4.052744
629.328684	5625.792718	7.984512	-0.120947	4.055580
629.682381	5633.798806	7.989517	-0.121018	4.058395
630.001154	5641.842359	7.994522	-0.121083	4.061220
630.521142	5649.778059	7.999526	-0.121185	4.064008
630.635366	5657.864776	8.004531	-0.121211	4.066842
630.670416	5665.906917	8.009536	-0.121223	4.069656
631.087087	5673.914784	8.014541	-0.121306	4.072462
631.426057	5681.861831	8.019546	-0.121374	4.075244
632.004118	5689.867293	8.024550	-0.121487	4.078047
632.508139	5697.888687	8.029555	-0.121586	4.080853
633.023083	5705.828499	8.034560	-0.121687	4.083629
632.851778	5714.010417	8.039565	-0.121661	4.086478
633.337934	5721.956363	8.044570	-0.121757	4.089251
633.986553	5729.997471	8.049574	-0.121883	4.092058
634.206063	5738.047941	8.054579	-0.121929	4.094861
634.516003	5746.010574	8.059584	-0.121992	4.097632
635.004962	5754.039154	8.064589	-0.122088	4.100426
635.292210	5762.032709	8.069594	-0.122147	4.103204
635.243261	5770.152065	8.074598	-0.122143	4.106019
635.767452	5778.129519	8.079603	-0.122246	4.108790
636.223176	5786.132357	8.084608	-0.122336	4.111567
637.103379	5794.071294	8.089613	-0.122505	4.114326
637.336212	5802.132728	8.094618	-0.122554	4.117117
637.746974	5810.152322	8.099622	-0.122635	4.119894
637.806755	5818.209737	8.104627	-0.122652	4.122677
638.490219	5826.130672	8.109632	-0.122784	4.125419
639.035231	5834.207234	8.114637	-0.122891	4.128212
639.421856	5842.236477	8.119642	-0.122968	4.130984
639.190967	5850.331270	8.124646	-0.122931	4.133769
639.371386	5858.382746	8.129651	-0.122969	4.136542
639.754984	5866.288811	8.134656	-0.123046	4.139266
640.037939	5874.356563	8.139661	-0.123104	4.142042
639.929902	5882.306687	8.144666	-0.123089	4.144771
640.689205	5890.326365	8.149670	-0.123236	4.147533
640.961829	5898.426478	8.154675	-0.123292	4.150315
641.003165	5906.424659	8.159680	-0.123305	4.153057
641.482065	5914.497468	8.164685	-0.123399	4.155828
641.499320	5922.444307	8.169690	-0.123408	4.158549
641.788104	5930.508290	8.174694	-0.123467	4.161311
641.973430	5938.445236	8.179699	-0.123506	4.164026
642.388272	5946.496522	8.184704	-0.123589	4.166782
642.167827	5954.571502	8.189709	-0.123553	4.169536
642.988494	5962.529184	8.194714	-0.123711	4.172261
643.546134	5970.530667	8.199718	-0.123820	4.174995
643.241805	5978.634591	8.204723	-0.123769	4.177753
643.277441	5986.644279	8.209728	-0.123781	4.180481
643.606163	5994.630156	8.214733	-0.123847	4.183202
644.260840	6002.602286	8.219738	-0.123974	4.185920
644.050012	6010.728838	8.224742	-0.123940	4.188679
644.819770	6018.710781	8.229747	-0.124089	4.191399
644.966216	6026.737888	8.234752	-0.124121	4.194124
644.676055	6034.850740	8.239757	-0.124073	4.196873
644.795588	6042.752882	8.244762	-0.124100	4.199552
645.198166	6050.790285	8.249766	-0.124180	4.202279
645.465517	6058.794946	8.254771	-0.124235	4.204991
646.050563	6066.720983	8.259776	-0.124350	4.207679
646.694545	6074.769657	8.264781	-0.124475	4.210407
647.094208	6082.756578	8.269786	-0.124554	4.213109
647.014080	6090.876551	8.274790	-0.124545	4.215849
647.063564	6098.896887	8.279795	-0.124559	4.218556
647.338767	6106.934008	8.284800	-0.124616	4.221269
647.418490	6114.892469	8.289805	-0.124636	4.223951
647.785463	6122.877941	8.294810	-0.124709	4.226644
648.182566	6130.907663	8.299814	-0.124789	4.229350
648.117422	6139.013154	8.304819	-0.124782	4.232075
648.129786	6146.995174	8.309824	-0.124789	4.234758
648.674103	6155.030745	8.314829	-0.124896	4.237462
648.842945	6162.961719	8.319834	-0.124933	4.240126
649.593837	6170.899446	8.324838	-0.125078	4.242796
650.049644	6178.983305	8.329843	-0.125168	4.245510
650.073627	6187.014072	8.334848	-0.125177	4.248201
650.314667	6195.110927	8.339853	-0.125228	4.250914
650.025263	6203.112328	8.344858	-0.125179	4.253588
650.340474	6211.170778	8.349862	-0.125243	4.256285
650.736968	6219.120055	8.354867	-0.125322	4.258945
650.731113	6227.157631	8.359872	-0.125326	4.261629
650.755456	6235.175119	8.364877	-0.125336	4.264305
651.455472	6243.142679	8.369882	-0.125472	4.266969
651.504602	6251.159403	8.374886	-0.125486	4.269641
652.084929	6259.161247	8.379891	-0.125599	4.272312
652.237257	6267.229507	8.384896	-0.125633	4.274999
652.056073	6275.314580	8.389901	-0.125604	4.277687
652.444052	6283.286352	8.394906	-0.125682	4.280341
652.757981	6291.232273	8.399910	-0.125746	4.282983
652.861868	6299.308136	8.404915	-0.125770	4.285666
653.210116	6307.253880	8.409920	-0.125840	4.288306
653.367105	6315.382834	8.414925	-0.125875	4.291003
653.662461	6323.350445	8.419930	-0.125935	4.293646
653.429394	6331.483481	8.424934	-0.125897	4.296337
653.846612	6339.409994	8.429939	-0.125980	4.298965
653.168267	6347.546157	8.434944	-0.125859	4.301651
654.083997	6355.394789	8.439949	-0.126035	4.304253
654.229257	6363.506481	8.444954	-0.126067	4.306934
654.550159	6371.465821	8.449958	-0.126132	4.309564
654.786001	6379.521166	8.454963	-0.126181	4.312224
654.714133	6387.481898	8.459968	-0.126173	4.314849
655.426399	6395.512339	8.464973	-0.126311	4.317501
655.667132	6403.442423	8.469978	-0.126361	4.320115
655.944363	6411.483777	8.474982	-0.126418	4.322764
656.314882	6419.473925	8.479987	-0.126492	4.325395
656.360009	6427.571512	8.484992	-0.126506	4.328058
656.014431	6435.723821	8.489997	-0.126447	4.330734
656.064769	6443.664822	8.495002	-0.126461	4.333341
656.873439	6451.607102	8.500006	-0.126617	4.335954
657.010414	6459.600728	8.505011	-0.126648	4.338576
656.577929	6467.747944	8.510016	-0.126573	4.341243
656.600603	6475.703283	8.515021	-0.126582	4.343849
657.113253	6483.654815	8.520026	-0.126683	4.346456
657.145263	6491.712233	8.525030	-0.126694	4.349092
656.934758	6499.851305	8.530035	-0.126660	4.351751
657.260573	6507.784340	8.535040	-0.126726	4.354346
657.766493	6515.832327	8.540045	-0.126825	4.356977
657.991254	6523.744738	8.545050	-0.126872	4.359561
658.626177	6531.761823	8.550054	-0.126996	4.362180
658.919638	6539.717072	8.555059	-0.127056	4.364775
659.116710	6547.771128	8.560064	-0.127098	4.367400
659.651538	6555.808123	8.565069	-0.127203	4.370020
660.513349	6563.807324	8.570074	-0.127368	4.372628
660.398699	6571.880426	8.575079	-0.127352	4.375253
661.028303	6579.860525	8.580083	-0.127475	4.377850
660.418945	6587.987301	8.585088	-0.127366	4.380485
660.697516	6596.004958	8.590093	-0.127424	4.383090
660.911568	6603.983448	8.595098	-0.127469	4.385679
661.202863	6611.958590	8.600103	-0.127528	4.388266
661.794492	6620.024695	8.605107	-0.127644	4.390883
661.659216	6628.062581	8.610112	-0.127624	4.393485
661.917260	6636.106904	8.615117	-0.127677	4.396090
662.338861	6644.038336	8.620122	-0.127761	4.398657
662.538495	6652.138811	8.625127	-0.127803	4.401276
662.556816	6660.095522	8.630131	-0.127812	4.403847
662.351169	6668.194180	8.635136	-0.127779	4.406460
662.633378	6676.265210	8.640141	-0.127837	4.409066
663.254848	6684.203812	8.645146	-0.127958	4.411629
663.415402	6692.167416	8.650151	-0.127993	4.414196
663.552695	6700.279609	8.655155	-0.128024	4.416810
663.865779	6708.212437	8.660160	-0.128087	4.419365
663.946288	6716.320625	8.665165	-0.128107	4.421973
663.911947	6724.308181	8.670170	-0.128106	4.424541
664.341696	6732.292271	8.675175	-0.128191	4.427109
664.839587	6740.298619	8.680179	-0.128289	4.429682
664.850017	6748.354103	8.685184	-0.128297	4.432268
665.004181	6756.391733	8.690189	-0.128331	4.434846
665.227992	6764.351262	8.695194	-0.128377	4.437399
665.618589	6772.338416	8.700199	-0.128455	4.439960
665.869335	6780.386948	8.705203	-0.128507	4.442538
666.366706	6788.332391	8.710208	-0.128605	4.445083
666.017393	6796.473942	8.715213	-0.128546	4.447685
666.389786	6804.422724	8.720218	-0.128620	4.450227
666.874916	6812.437264	8.725223	-0.128716	4.452789
666.907720	6820.507590	8.730227	-0.128727	4.455366
667.200196	6828.459822	8.735232	-0.128787	4.457904
668.009259	6836.439475	8.740237	-0.128943	4.460452
668.204161	6844.469982	8.745242	-0.128984	4.463012
668.200065	6852.603743	8.750247	-0.128989	4.465603
668.431019	6860.588281	8.755251	-0.129037	4.468145
668.743921	6868.602985	8.760256	-0.129100	4.470696
669.019875	6876.559975	8.765261	-0.129157	4.473227
669.090169	6884.592773	8.770266	-0.129175	4.475780
669.462360	6892.599209	8.775271	-0.129250	4.478324
669.692294	6900.635565	8.780275	-0.129298	4.480876
669.678320	6908.597586	8.785280	-0.129301	4.483402
670.374903	6916.647997	8.790285	-0.129436	4.485956
670.862464	6924.641447	8.795290	-0.129532	4.488491
670.994053	6932.676866	8.800295	-0.129561	4.491036
671.259588	6940.706648	8.805299	-0.129616	4.493578
671.305217	6948.720596	8.810304	-0.129630	4.496113
671.670477	6956.716184	8.815309	-0.129703	4.498642
671.468123	6964.801970	8.820314	-0.129671	4.501196
671.773887	6972.745054	8.825319	-0.129733	4.503705
671.484787	6980.899086	8.830323	-0.129684	4.506278
671.835728	6988.809289	8.835328	-0.129755	4.508774
672.363926	6996.854202	8.840333	-0.129859	4.511311
672.475424	7004.791511	8.845338	-0.129884	4.513812
672.625268	7012.836091	8.850343	-0.129918	4.516346
672.793228	7020.854343	8.855347	-0.129954	4.518870
672.880514	7028.912556	8.860352	-0.129976	4.521405
673.083236	7036.849248	8.865357	-0.130019	4.523900
672.844376	7044.930984	8.870362	-0.129979	4.526438
673.429363	7052.843897	8.875367	-0.130094	4.528925
673.957054	7060.943920	8.880371	-0.130197	4.531468
673.982423	7068.892979	8.885376	-0.130207	4.533961
674.878638	7076.943014	8.890381	-0.130379	4.536486
674.579744	7084.946128	8.895386	-0.130329	4.538993
674.301802	7093.071106	8.900391	-0.130282	4.541536
674.812822	7100.978994	8.905395	-0.130383	4.544012
674.926672	7109.022642	8.910400	-0.130409	4.546528
675.466001	7117.016321	8.915405	-0.130515	4.549028
675.711914	7125.068283	8.920410	-0.130566	4.551544
676.136205	7133.039803	8.925415	-0.130650	4.554034
675.737339	7141.177376	8.930419	-0.130581	4.556573
676.131845	7149.035899	8.935424	-0.130660	4.559024
676.075566	7157.198583	8.940429	-0.130655	4.561569
676.459076	7165.054989	8.945434	-0.130731	4.564017
677.088043	7173.097176	8.950439	-0.130854	4.566522
677.047525	7181.142951	8.955443	-0.130851	4.569026
677.258255	7189.187061	8.960448	-0.130896	4.571528
677.770259	7197.173191	8.965453	-0.130996	4.574012
678.329795	7205.201887	8.970458	-0.131106	4.576507
678.373154	7213.175696	8.975463	-0.131119	4.578983
679.129871	7221.230922	8.980467	-0.131265	4.581483
679.041725	7229.171728	8.985472	-0.131254	4.583946
679.013307	7237.338216	8.990477	-0.131254	4.586478
679.630283	7245.243335	8.995482	-0.131374	4.588928
679.506201	7253.361590	9.000487	-0.131356	4.591442
679.426907	7261.378200	9.005491	-0.131347	4.593923
679.894084	7269.342385	9.010496	-0.131439	4.596387
679.688364	7277.356836	9.015501	-0.131406	4.598864
680.195924	7285.370194	9.020506	-0.131506	4.601341
680.786344	7293.287833	9.025511	-0.131621	4.603786
681.146266	7301.401472	9.030515	-0.131693	4.606291
681.265637	7309.334718	9.035520	-0.131721	4.608738
681.447787	7317.460563	9.040525	-0.131760	4.611243
681.986610	7325.388938	9.045530	-0.131866	4.613687
682.154463	7333.452774	9.050535	-0.131902	4.616170
682.045917	7341.473466	9.055539	-0.131887	4.618639
682.063801	7349.495339	9.060544	-0.131896	4.621107
682.765757	7357.447339	9.065549	-0.132032	4.623552
682.563178	7365.522592	9.070554	-0.131999	4.626034
683.061826	7373.477293	9.075559	-0.132097	4.628477
683.516549	7381.571671	9.080563	-0.132187	4.630962
683.755923	7389.515719	9.085568	-0.132237	4.633399
683.404352	7397.659025	9.090573	-0.132177	4.635897
683.806606	7405.579207	9.095578	-0.132257	4.638324
683.959766	7413.649153	9.100583	-0.132291	4.640796
684.184879	7421.596081	9.105587	-0.132338	4.643229
684.680993	7429.616111	9.110592	-0.132435	4.645683
684.783340	7437.682717	9.115597	-0.132460	4.648150
684.849436	7445.702500	9.120602	-0.132477	4.650601
685.124967	7453.660589	9.125607	-0.132534	4.653032
685.272954	7461.756611	9.130611	-0.132567	4.655504
685.188569	7469.775539	9.135616	-0.132556	4.657952
685.343582	7477.795256	9.140621	-0.132590	4.660398
685.552887	7485.737475	9.145626	-0.132635	4.662819
686.170307	7493.695498	9.150631	-0.132755	4.665243
685.578345	7501.912110	9.155635	-0.132650	4.667746
686.223058	7509.871726	9.160640	-0.132775	4.670168
686.194867	7517.958363	9.165645	-0.132775	4.672628
686.567806	7525.900940	9.170650	-0.132850	4.675043
686.667264	7533.924707	9.175655	-0.132874	4.677481
686.993952	7541.877639	9.180659	-0.132940	4.679896
686.950137	7549.847491	9.185664	-0.132937	4.682316
687.875610	7557.816892	9.190669	-0.133114	4.684732
687.707525	7565.917068	9.195674	-0.133088	4.687189
687.740988	7573.963765	9.200679	-0.133100	4.689628
687.765388	7582.054825	9.205683	-0.133110	4.692079
687.844819	7589.977175	9.210688	-0.133130	4.694478
688.913560	7597.956849	9.215693	-0.133334	4.696891
688.567633	7606.029574	9.220698	-0.133275	4.699333
688.639585	7614.127566	9.225703	-0.133293	4.701781
689.007736	7622.075654	9.230707	-0.133367	4.704182
689.461306	7630.080221	9.235712	-0.133457	4.706598
689.855949	7638.019365	9.240717	-0.133536	4.708994
690.013705	7646.123570	9.245722	-0.133570	4.711438
690.115683	7654.071120	9.250727	-0.133594	4.713835
690.540077	7662.162965	9.255731	-0.133679	4.716272
691.120827	7670.073740	9.260736	-0.133792	4.718654
691.332469	7678.201625	9.265741	-0.133837	4.721100
691.453997	7686.147322	9.270746	-0.133865	4.723491
691.716336	7694.147055	9.275751	-0.133919	4.725896
691.811718	7702.257620	9.280755	-0.133942	4.728333
692.043409	7710.256127	9.285760	-0.133990	4.730736
692.394867	7718.287929	9.290765	-0.134061	4.733147
692.856585	7726.225069	9.295770	-0.134152	4.735527
692.895181	7734.302011	9.300775	-0.134165	4.737950
692.923382	7742.340307	9.305779	-0.134175	4.740360
693.846585	7750.224532	9.310784	-0.134352	4.742720
693.601407	7758.344583	9.315789	-0.134312	4.745153
693.975989	7766.371609	9.320794	-0.134387	4.747554
693.646034	7774.401962	9.325799	-0.134331	4.749958
693.869379	7782.479582	9.330803	-0.134378	4.752373
694.549482	7790.328008	9.335808	-0.134509	4.754717
694.639140	7798.427202	9.340813	-0.134531	4.757136
694.449593	7806.461618	9.345818	-0.134501	4.759535
694.947729	7814.442804	9.350823	-0.134599	4.761916
695.358247	7822.427190	9.355827	-0.134681	4.764296
695.275760	7830.472900	9.360832	-0.134671	4.766695
695.511915	7838.423672	9.365837	-0.134720	4.769063
695.776425	7846.566517	9.370842	-0.134775	4.771487
695.995858	7854.459197	9.375847	-0.134821	4.773836
696.094505	7862.580028	9.380851	-0.134844	4.776252
695.997325	7870.527199	9.385856	-0.134831	4.778615
696.236959	7878.606527	9.390861	-0.134881	4.781016
696.819665	7886.512590	9.395866	-0.134995	4.783362
696.942080	7894.609200	9.400871	-0.135023	4.785766
697.113394	7902.582213	9.405875	-0.135060	4.788132
697.178780	7910.625191	9.410880	-0.135078	4.790517
697.711155	7918.599604	9.415885	-0.135182	4.792879
697.688404	7926.644226	9.420890	-0.135183	4.795263
697.968627	7934.639126	9.425895	-0.135241	4.797630
698.199209	7942.670082	9.430899	-0.135289	4.800006
698.661446	7950.668362	9.435904	-0.135380	4.802371
698.397672	7958.682297	9.440909	-0.135336	4.804742
698.670860	7966.726036	9.445914	-0.135392	4.807119
698.859648	7974.721864	9.450919	-0.135433	4.809480
699.483341	7982.788614	9.455923	-0.135554	4.811859
700.106262	7990.088288	9.460928	-0.135675	4.814011
699.986582	7994.807952	9.465933	-0.135656	4.815404

700.142174	7997.437330	9.470938	-0.135686	4.816179
699.965081	7998.724909	9.475943	-0.135654	4.816560
700.212264	7999.138453	9.480947	-0.135701	4.816680
700.678948	8000.132421	9.485952	-0.135788	4.816971
700.648121	8000.199695	9.490957	-0.135783	4.816991
700.946364	8000.171557	9.495962	-0.135838	4.816982
700.797710	8000.205222	9.500967	-0.135810	4.816992
701.415989	8000.163050	9.505971	-0.135926	4.816977
701.066815	8000.166043	9.510976	-0.135861	4.816980
701.355189	8000.218212	9.515981	-0.135914	4.816994
701.298023	8000.190850	9.520986	-0.135904	4.816986
701.386152	8000.148828	9.525991	-0.135920	4.816973
701.309350	8000.222793	9.530995	-0.135906	4.816995
701.829204	8000.112379	9.536000	-0.136003	4.816960
701.548330	8000.242429	9.541005	-0.135950	4.817000
701.382538	8000.247240	9.546010	-0.135920	4.817002
701.627006	8000.179087	9.551015	-0.135965	4.816981
702.042171	8000.203604	9.556019	-0.136042	4.816986
702.501893	8000.088012	9.561024	-0.136128	4.816950
702.305213	8000.145274	9.566029	-0.136091	4.816968
702.538480	8000.088591	9.571034	-0.136135	4.816950
702.516215	8000.059658	9.576039	-0.136131	4.816941
702.302515	8000.219349	9.581043	-0.136091	4.816990
702.913591	8000.094487	9.586048	-0.136205	4.816950
702.539682	8000.188139	9.591053	-0.136135	4.816979
702.879918	8000.123608	9.596058	-0.136199	4.816959
703.282231	8000.092872	9.601063	-0.136274	4.816948
703.228709	8000.147088	9.606067	-0.136264	4.816964
703.077848	8000.107665	9.611072	-0.136236	4.816953
703.293141	8000.096226	9.616077	-0.136276	4.816949
703.450642	8000.129406	9.621082	-0.136305	4.816958
703.099394	8000.111187	9.626087	-0.136240	4.816954
703.606896	8000.117042	9.631091	-0.136334	4.816953
703.586094	8000.074368	9.636096	-0.136330	4.816941
703.415342	8000.134154	9.641101	-0.136299	4.816959
703.305966	8000.128204	9.646106	-0.136278	4.816958
702.976515	8000.229965	9.651111	-0.136217	4.816990
703.295981	8000.186283	9.656115	-0.136276	4.816975
703.251032	8000.111467	9.661120	-0.136268	4.816953
703.294857	8000.122745	9.666125	-0.136276	4.816956
703.635516	8000.086807	9.671130	-0.136340	4.816944
703.540388	8000.067316	9.676135	-0.136322	4.816939
703.531119	8000.187870	9.681139	-0.136320	4.816975
703.384573	8000.172866	9.686144	-0.136293	4.816971
703.843043	8000.115486	9.691149	-0.136378	4.816952
704.010459	8000.085296	9.696154	-0.136410	4.816942
703.986008	8000.127265	9.701159	-0.136405	4.816955
703.946475	8000.166879	9.706163	-0.136398	4.816966
703.838519	8000.084720	9.711168	-0.136378	4.816943
703.949119	8000.194453	9.716173	-0.136398	4.816975
704.406920	8000.148710	9.721178	-0.136484	4.816959
704.417817	8000.106533	9.726183	-0.136486	4.816946
704.563970	8000.118360	9.731187	-0.136513	4.816949
704.751325	8000.065192	9.736192	-0.136548	4.816933
704.551301	8000.164752	9.741197	-0.136511	4.816963
704.363911	8000.172398	9.746202	-0.136476	4.816966
704.005431	8000.079949	9.751207	-0.136409	4.816941
704.625298	8000.092866	9.756211	-0.136524	4.816941
704.302547	8000.136501	9.761216	-0.136464	4.816956
704.412312	8000.125523	9.766221	-0.136485	4.816952
704.484370	8000.169008	9.771226	-0.136498	4.816965
704.325059	8000.133685	9.776231	-0.136469	4.816955
704.228632	8000.230638	9.781235	-0.136451	4.816984
704.208950	8000.197509	9.786240	-0.136447	4.816974
704.436298	8000.185203	9.791245	-0.136490	4.816970
704.242576	8000.190631	9.796250	-0.136454	4.816972
704.423038	8000.145824	9.801255	-0.136487	4.816958
704.327818	8000.287265	9.806259	-0.136469	4.817000
704.286042	8000.204026	9.811264	-0.136462	4.816976
704.503695	8000.222272	9.816269	-0.136502	4.816980
704.587623	8000.242651	9.821274	-0.136518	4.816986
704.769001	8000.175624	9.826279	-0.136552	4.816965
704.508397	8000.247763	9.831283	-0.136503	4.816988
704.164030	8000.284705	9.836288	-0.136439	4.817000
704.242075	8000.294404	9.841293	-0.136454	4.817003
704.156936	8000.310009	9.846298	-0.136438	4.817008
704.334474	8000.232334	9.851303	-0.136471	4.816984
704.636801	8000.234970	9.856307	-0.136527	4.816983
704.247883	8000.230978	9.861312	-0.136455	4.816984
704.565575	8000.185152	9.866317	-0.136514	4.816969
705.069801	8000.183550	9.871322	-0.136608	4.816966
704.987268	8000.128257	9.876327	-0.136593	4.816950
705.353800	8000.110727	9.881331	-0.136661	4.816943
705.214536	8000.066189	9.886336	-0.136635	4.816931
705.419951	8000.077890	9.891341	-0.136673	4.816933
704.984089	8000.222448	9.896346	-0.136592	4.816978
705.064900	8000.145370	9.901351	-0.136607	4.816955
705.143120	8000.134955	9.906355	-0.136622	4.816951
705.232183	8000.140593	9.911360	-0.136638	4.816953
704.631008	8000.195732	9.916365	-0.136527	4.816972
704.451682	8000.264913	9.921370	-0.136493	4.816993
704.318057	8000.300932	9.926375	-0.136468	4.817004
704.684645	8000.282344	9.931379	-0.136537	4.816997
705.076680	8000.133925	9.936384	-0.136610	4.816951
705.327469	8000.205632	9.941389	-0.136656	4.816971
705.861919	8000.176979	9.946394	-0.136756	4.816961
705.662174	8000.121960	9.951399	-0.136719	4.816945
705.414404	8000.225006	9.956403	-0.136673	4.816977
705.514693	8000.211761	9.961408	-0.136691	4.816972
705.923890	8000.145140	9.966413	-0.136767	4.816951
705.241450	8000.244528	9.971418	-0.136641	4.816983
705.226937	8000.231597	9.976423	-0.136638	4.816980
705.170398	8000.249769	9.981427	-0.136627	4.816985
705.386951	8000.073180	9.986432	-0.136668	4.816932
705.478239	8000.161439	9.991437	-0.136685	4.816958
705.636659	8000.141697	9.996442	-0.136714	4.816951
705.128083	8000.222643	10.001447	-0.136620	4.816977
705.454246	8000.226714	10.006451	-0.136680	4.816977
705.586203	8000.177969	10.011456	-0.136705	4.816962
705.336712	8000.203695	10.016461	-0.136658	4.816971
705.514095	8000.185310	10.021466	-0.136692	4.816965
705.732003	8000.130504	10.026471	-0.136732	4.816947
705.706825	8000.245520	10.031475	-0.136727	4.816981
705.590935	8000.184408	10.036480	-0.136706	4.816964
705.783412	8000.180025	10.041485	-0.136742	4.816962
705.667334	8000.307376	10.046490	-0.136720	4.817000
705.228226	8000.286710	10.051495	-0.136639	4.816996
705.918821	8000.196984	10.056499	-0.136767	4.816966
705.684387	8000.217653	10.061504	-0.136723	4.816973
705.399499	8000.296821	10.066509	-0.136670	4.816998
705.507752	8000.283703	10.071514	-0.136691	4.816994
705.748033	8000.154073	10.076519	-0.136735	4.816954
705.346290	8000.281169	10.081523	-0.136661	4.816994
704.917523	8000.285018	10.086528	-0.136581	4.816997
705.483205	8000.225092	10.091533	-0.136686	4.816976
705.992504	8000.166397	10.096538	-0.136781	4.816957
705.860805	8000.146329	10.101543	-0.136756	4.816951
705.496698	8000.224252	10.106547	-0.136689	4.816976
705.757606	8000.159534	10.111552	-0.136737	4.816956
705.963615	8000.165952	10.116557	-0.136776	4.816957
706.045427	8000.237123	10.121562	-0.136791	4.816977
706.062636	8000.172808	10.126567	-0.136794	4.816958
706.363472	8000.227306	10.131571	-0.136850	4.816973
706.226073	8000.189147	10.136576	-0.136825	4.816962
705.729881	8000.279817	10.141581	-0.136732	4.816991
706.101998	8000.298377	10.146586	-0.136802	4.816995
705.713843	8000.300745	10.151591	-0.136730	4.816998
706.269821	8000.243845	10.156595	-0.136833	4.816978
706.690765	8000.144585	10.161600	-0.136911	4.816947
706.894817	8000.156268	10.166605	-0.136949	4.816950
706.381158	8000.192662	10.171610	-0.136854	4.816963
706.169570	8000.197807	10.176615	-0.136814	4.816965
706.527214	8000.204493	10.181619	-0.136881	4.816965
706.470085	8000.166538	10.186624	-0.136870	4.816955
706.202581	8000.249156	10.191629	-0.136821	4.816980
706.052938	8000.265864	10.196634	-0.136793	4.816986
705.882531	8000.242010	10.201639	-0.136761	4.816980
705.899918	8000.246521	10.206643	-0.136764	4.816981
706.221381	8000.156286	10.211648	-0.136824	4.816953
706.216203	8000.185853	10.216653	-0.136823	4.816961
706.687469	8000.155150	10.221658	-0.136911	4.816950
706.435846	8000.191430	10.226663	-0.136864	4.816962
707.087646	8000.138155	10.231667	-0.136986	4.816943
707.092828	8000.111768	10.236672	-0.136987	4.816936
706.946543	8000.142293	10.241677	-0.136959	4.816945
706.484248	8000.279024	10.246682	-0.136873	4.816988
705.996437	8000.280884	10.251687	-0.136783	4.816990
706.337972	8000.249199	10.256691	-0.136846	4.816980
706.125250	8000.249032	10.261696	-0.136807	4.816980
706.998628	8000.123006	10.266701	-0.136969	4.816939
706.710146	8000.166118	10.271706	-0.136916	4.816953
706.412357	8000.218613	10.276711	-0.136860	4.816970
706.617179	8000.204896	10.281715	-0.136898	4.816965
706.163026	8000.305755	10.286720	-0.136814	4.816997
706.565322	8000.219968	10.291725	-0.136889	4.816970
706.219369	8000.290764	10.296730	-0.136824	4.816992
706.597511	8000.219420	10.301735	-0.136895	4.816970
706.554138	8000.248387	10.306739	-0.136887	4.816978
706.179793	8000.272149	10.311744	-0.136817	4.816987
706.431259	8000.210459	10.316749	-0.136864	4.816968
706.354908	8000.230437	10.321754	-0.136850	4.816974
706.323616	8000.175947	10.326759	-0.136844	4.816958
706.938284	8000.162323	10.331763	-0.136958	4.816951
706.392464	8000.240564	10.336768	-0.136857	4.816977
706.360967	8000.185012	10.341773	-0.136851	4.816961
706.564771	8000.162808	10.346778	-0.136889	4.816953
706.307586	8000.186295	10.351783	-0.136841	4.816961
706.723231	8000.223541	10.356787	-0.136919	4.816970
706.550756	8000.236713	10.361792	-0.136886	4.816975
706.737655	8000.208949	10.366797	-0.136921	4.816966
706.494699	8000.253836	10.371802	-0.136876	4.816980
706.756418	8000.152072	10.376807	-0.136925	4.816949
707.120757	8000.147217	10.381811	-0.136993	4.816946
706.349854	8000.236741	10.386816	-0.136849	4.816976
706.282439	8000.263212	10.391821	-0.136837	4.816984
706.071580	8000.329780	10.396826	-0.136797	4.817005
706.058503	8000.295695	10.401831	-0.136795	4.816995
706.058045	8000.353925	10.406835	-0.136795	4.817012
706.429996	8000.225307	10.411840	-0.136864	4.816972
706.490239	8000.276022	10.416845	-0.136876	4.816987
706.581637	8000.273227	10.421850	-0.136893	4.816985
706.709151	8000.221235	10.426855	-0.136916	4.816970
706.942041	8000.212194	10.431859	-0.136960	4.816966
707.123116	8000.156809	10.436864	-0.136993	4.816949
706.753416	8000.185938	10.441869	-0.136925	4.816959
706.732236	8000.236431	10.446874	-0.136921	4.816974
706.717604	8000.242556	10.451879	-0.136918	4.816976
707.042461	8000.260375	10.456883	-0.136979	4.816980
706.681651	8000.234583	10.461888	-0.136911	4.816974
706.442195	8000.282702	10.466893	-0.136867	4.816989
706.565573	8000.304763	10.471898	-0.136890	4.816995
706.250972	8000.340052	10.476903	-0.136831	4.817007
706.565377	8000.350294	10.481907	-0.136890	4.817008
706.656686	8000.282909	10.486912	-0.136907	4.816988
706.401560	8000.317015	10.491917	-0.136859	4.816999
706.661398	8000.258634	10.496922	-0.136908	4.816981
706.799967	8000.221639	10.501927	-0.136934	4.816969
706.241077	8000.351557	10.506931	-0.136830	4.817010
706.314120	8000.323061	10.511936	-0.136843	4.817001
706.394130	8000.325381	10.516941	-0.136858	4.817002
706.763153	8000.269776	10.521946	-0.136927	4.816984
706.858928	8000.258579	10.526951	-0.136945	4.816980
707.133217	8000.248073	10.531955	-0.136996	4.816975
707.138168	8000.228035	10.536960	-0.136997	4.816970
707.178391	8000.190552	10.541965	-0.137004	4.816958
707.247314	8000.276347	10.546970	-0.137017	4.816983
707.067087	8000.258689	10.551975	-0.136984	4.816979
706.761131	8000.369292	10.556979	-0.136927	4.817013
706.712118	8000.302875	10.561984	-0.136918	4.816994
706.697781	8000.284651	10.566989	-0.136915	4.816988
706.728853	8000.346555	10.571994	-0.136921	4.817006
706.740386	8000.302268	10.576999	-0.136923	4.816993
706.803748	8000.390092	10.582003	-0.136935	4.817019
706.666162	8000.360400	10.587008	-0.136909	4.817011
706.520529	8000.339052	10.592013	-0.136882	4.817005
706.618173	8000.333178	10.597018	-0.136900	4.817003
706.864162	8000.324345	10.602023	-0.136946	4.816999
706.978257	8000.333554	10.607027	-0.136967	4.817001
706.890612	8000.271824	10.612032	-0.136951	4.816984
707.064290	8000.249146	10.617037	-0.136984	4.816976
706.770025	8000.372639	10.622042	-0.136929	4.817014
706.585116	8000.360202	10.627047	-0.136894	4.817011
706.893271	8000.284581	10.632051	-0.136952	4.816987
706.774037	8000.340944	10.637056	-0.136930	4.817005
706.688179	8000.337477	10.642061	-0.136914	4.817004
706.864248	8000.320132	10.647066	-0.136946	4.816998
706.605820	8000.339363	10.652071	-0.136898	4.817005
706.693181	8000.382035	10.657075	-0.136915	4.817017
706.814985	8000.254775	10.662080	-0.136937	4.816979
706.867232	8000.300070	10.667085	-0.136947	4.816992
706.726753	8000.407982	10.672090	-0.136921	4.817025
707.217140	8000.303463	10.677095	-0.137012	4.816991
707.200057	8000.411200	10.682099	-0.137009	4.817023
707.120588	8000.423716	10.687104	-0.136994	4.817027
707.149710	8000.383941	10.692109	-0.137000	4.817015
706.885722	8000.420025	10.697114	-0.136951	4.817027
706.981994	8000.371776	10.702119	-0.136969	4.817013
707.457423	8000.379261	10.707123	-0.137057	4.817013
707.528909	8000.302033	10.712128	-0.137071	4.816990
707.106627	8000.294331	10.717133	-0.136992	4.816989
707.571680	8000.257180	10.722138	-0.137079	4.816976
707.048557	8000.317775	10.727143	-0.136981	4.816996
707.038201	8000.389617	10.732147	-0.136979	4.817018
706.916135	8000.371815	10.737152	-0.136957	4.817013
707.065531	8000.340285	10.742157	-0.136984	4.817003
707.179330	8000.329372	10.747162	-0.137006	4.816999
707.179113	8000.318783	10.752167	-0.137006	4.816996
707.342590	8000.336182	10.757171	-0.137036	4.817000
706.842075	8000.374897	10.762176	-0.136943	4.817014
707.059139	8000.381492	10.767181	-0.136983	4.817015
707.528174	8000.344404	10.772186	-0.137071	4.817002
707.965864	8000.206231	10.777191	-0.137152	4.816959
707.502512	8000.300591	10.782195	-0.137066	4.816989
707.465183	8000.324360	10.787200	-0.137059	4.816996
707.676706	8000.267336	10.792205	-0.137099	4.816979
707.661416	8000.281922	10.797210	-0.137096	4.816983
707.666173	8000.287293	10.802215	-0.137097	4.816985
707.802392	8000.262968	10.807219	-0.137122	4.816977
707.679440	8000.273742	10.812224	-0.137099	4.816980
707.442148	8000.242480	10.817229	-0.137055	4.816972
707.509353	8000.310247	10.822234	-0.137068	4.816992
708.116073	8000.187441	10.827239	-0.137180	4.816953
708.648741	8000.158767	10.832243	-0.137280	4.816942
708.741640	8000.176115	10.837248	-0.137297	4.816947
708.577208	8000.226473	10.842253	-0.137266	4.816962
708.782954	8000.203243	10.847258	-0.137305	4.816955
708.806604	8000.125260	10.852263	-0.137309	4.816931
708.980473	8000.137530	10.857267	-0.137342	4.816934
709.073520	8000.082876	10.862272	-0.137359	4.816918
708.655517	8000.125007	10.867277	-0.137281	4.816932
708.389481	8000.252122	10.872282	-0.137232	4.816971
708.611592	8000.104201	10.877287	-0.137273	4.816926
708.452883	8000.181121	10.882291	-0.137243	4.816950
708.387758	8000.167392	10.887296	-0.137231	4.816946
708.457019	8000.156837	10.892301	-0.137244	4.816942
708.266990	8000.244911	10.897306	-0.137209	4.816969
708.346192	8000.148744	10.902311	-0.137224	4.816941
708.523012	8000.216121	10.907315	-0.137257	4.816960
708.195558	8000.181320	10.912320	-0.137196	4.816951
707.970184	8000.232836	10.917325	-0.137154	4.816967
708.154291	8000.284444	10.922330	-0.137188	4.816981
708.276246	8000.188950	10.927335	-0.137211	4.816953
708.692652	8000.158447	10.932339	-0.137288	4.816942
708.795276	8000.151594	10.937344	-0.137308	4.816939
708.966771	8000.108764	10.942349	-0.137339	4.816926
708.971372	8000.143782	10.947354	-0.137340	4.816936
709.008893	8000.099902	10.952359	-0.137347	4.816923
708.906053	8000.142758	10.957363	-0.137328	4.816936
708.964352	8000.105559	10.962368	-0.137339	4.816925
709.043896	8000.076106	10.967373	-0.137354	4.816916
708.804010	8000.127394	10.972378	-0.137309	4.816932
709.143371	8000.103090	10.977383	-0.137373	4.816923
708.871771	8000.128465	10.982387	-0.137322	4.816932
708.934082	8000.127331	10.987392	-0.137334	4.816931
708.551853	8000.173201	10.992397	-0.137263	4.816947
708.722348	8000.221419	10.997402	-0.137294	4.816960
708.451716	8000.209748	11.002407	-0.137244	4.816958
709.143929	8000.136997	11.007411	-0.137373	4.816933
708.835761	8000.145913	11.012416	-0.137315	4.816937
708.888349	8000.123448	11.017421	-0.137325	4.816931
709.027500	8000.129877	11.022426	-0.137351	4.816932
709.224373	8000.126625	11.027431	-0.137388	4.816930
709.236781	8000.146942	11.032435	-0.137390	4.816936
708.852450	8000.149364	11.037440	-0.137319	4.816938
708.892224	8000.120344	11.042445	-0.137326	4.816930
708.971835	8000.161837	11.047450	-0.137341	4.816941
708.968078	8000.069658	11.052455	-0.137340	4.816914
708.832614	8000.152238	11.057459	-0.137315	4.816939
708.719913	8000.183291	11.062464	-0.137294	4.816949
708.847052	8000.133410	11.067469	-0.137318	4.816934
708.948110	8000.169947	11.072474	-0.137337	4.816944
709.279678	8000.096812	11.077479	-0.137398	4.816921
709.161802	8000.154256	11.082483	-0.137377	4.816938
708.637310	8000.216946	11.087488	-0.137279	4.816959
708.602416	8000.203692	11.092493	-0.137273	4.816956
708.652327	8000.257424	11.097498	-0.137282	4.816971
708.743312	8000.147677	11.102503	-0.137299	4.816938
708.731201	8000.212080	11.107507	-0.137297	4.816957
708.680363	8000.277992	11.112512	-0.137287	4.816977
708.722062	8000.192881	11.117517	-0.137295	4.816952
708.864334	8000.190888	11.122522	-0.137321	4.816951
708.898506	8000.190369	11.127527	-0.137328	4.816950
708.850451	8000.194909	11.132531	-0.137319	4.816952
709.002194	8000.181418	11.137536	-0.137347	4.816947
709.257075	8000.176962	11.142541	-0.137395	4.816945
709.300128	8000.183996	11.147546	-0.137403	4.816946
708.823332	8000.212493	11.152551	-0.137314	4.816957
708.370005	8000.286892	11.157555	-0.137230	4.816981
708.492596	8000.294119	11.162560	-0.137253	4.816983
708.244140	8000.248913	11.167565	-0.137206	4.816970
708.483372	8000.299272	11.172570	-0.137251	4.816984
708.301169	8000.292171	11.177575	-0.137217	4.816983
708.323901	8000.296766	11.182579	-0.137221	4.816984
708.586175	8000.216188	11.187584	-0.137270	4.816959
707.945991	8000.338471	11.192589	-0.137151	4.816998
708.834474	8000.238103	11.197594	-0.137316	4.816965
708.489061	8000.244314	11.202599	-0.137252	4.816968
708.363539	8000.285755	11.207603	-0.137229	4.816981
707.946528	8000.343783	11.212608	-0.137151	4.817000
707.855642	8000.369886	11.217613	-0.137134	4.817008
707.912258	8000.379250	11.222618	-0.137145	4.817010
708.252515	8000.293546	11.227623	-0.137208	4.816984
708.430507	8000.370472	11.232627	-0.137241	4.817005
708.476734	8000.279080	11.237632	-0.137250	4.816978
708.925042	8000.161192	11.242637	-0.137333	4.816941
708.887090	8000.258015	11.247642	-0.137326	4.816970
708.993153	8000.122032	11.252647	-0.137346	4.816930
709.080720	8000.180593	11.257651	-0.137362	4.816946
708.897317	8000.202062	11.262656	-0.137328	4.816954
708.633965	8000.221213	11.267661	-0.137279	4.816961
708.928762	8000.204679	11.272666	-0.137334	4.816954
708.943855	8000.176329	11.277671	-0.137337	4.816946
708.893775	8000.205192	11.282675	-0.137328	4.816955
709.171446	8000.171446	11.287680	-0.137380	4.816943
708.893903	8000.203081	11.292685	-0.137328	4.816954
708.868966	8000.264106	11.297690	-0.137323	4.816972
708.489814	8000.224255	11.302695	-0.137253	4.816962
708.688304	8000.208322	11.307699	-0.137290	4.816956
708.745092	8000.198630	11.312704	-0.137300	4.816953
708.976399	8000.192744	11.317709	-0.137343	4.816951
708.948306	8000.227247	11.322714	-0.137338	4.816961
709.376620	8000.177873	11.327719	-0.137418	4.816944
709.667689	8000.148574	11.332723	-0.137472	4.816934
709.224815	8000.200900	11.337728	-0.137390	4.816952
709.454578	8000.142046	11.342733	-0.137433	4.816933
709.156883	8000.182893	11.347738	-0.137377	4.816947
708.774606	8000.242527	11.352743	-0.137306	4.816966
708.907293	8000.239324	11.357747	-0.137331	4.816965
709.006168	8000.240884	11.362752	-0.137349	4.816965
709.198888	8000.151797	11.367757	-0.137385	4.816937
709.171073	8000.211718	11.372762	-0.137380	4.816955
708.792914	8000.202590	11.377767	-0.137310	4.816954
709.441666	8000.121743	11.382771	-0.137430	4.816927
709.435749	8000.107886	11.387776	-0.137429	4.816923
709.424766	8000.119363	11.392781	-0.137427	4.816927
709.676579	8000.138156	11.397786	-0.137474	4.816931
709.412739	8000.117061	11.402791	-0.137425	4.816926
709.318862	8000.159000	11.407795	-0.137408	4.816939
709.813668	8000.109614	11.412800	-0.137500	4.816922
709.938848	8000.095704	11.417805	-0.137523	4.816917
709.925541	8000.127264	11.422810	-0.137521	4.816927
709.516024	8000.215059	11.427815	-0.137445	4.816955
709.471037	8000.226001	11.432819	-0.137436	4.816958
709.512580	8000.170536	11.437824	-0.137444	4.816941
709.561993	8000.112018	11.442829	-0.137453	4.816924
709.586011	8000.168520	11.447834	-0.137458	4.816941
709.528773	8000.116794	11.452839	-0.137447	4.816926
709.265812	8000.188896	11.457843	-0.137398	4.816948
709.524929	8000.171801	11.462848	-0.137446	4.816942
709.334193	8000.147621	11.467853	-0.137411	4.816936
709.216001	8000.175412	11.472858	-0.137389	4.816944
709.228125	8000.126896	11.477863	-0.137391	4.816930
709.392440	8000.129486	11.482867	-0.137422	4.816930
709.478935	8000.120261	11.487872	-0.137438	4.816927
709.016991	8000.126755	11.492877	-0.137352	4.816931
709.485111	8000.126716	11.497882	-0.137439	4.816929
709.114675	8000.096532	11.502887	-0.137370	4.816921
709.046993	8000.169590	11.507891	-0.137358	4.816943
709.298006	8000.117424	11.512896	-0.137404	4.816927
709.256254	8000.162301	11.517901	-0.137397	4.816940
709.314419	8000.163219	11.522906	-0.137407	4.816940
709.531158	8000.068158	11.527911	-0.137448	4.816911
709.389544	8000.126287	11.532915	-0.137421	4.816929
709.711050	8000.098526	11.537920	-0.137481	4.816919
709.192798	8000.099898	11.542925	-0.137385	4.816922
709.538741	8000.141350	11.547930	-0.137449	4.816933
709.321711	8000.129464	11.552935	-0.137409	4.816930
709.746530	8000.105448	11.557939	-0.137488	4.816921
709.827489	8000.076017	11.562944	-0.137503	4.816912
709.620008	8000.105578	11.567949	-0.137465	4.816922
709.552964	8000.130997	11.572954	-0.137452	4.816930
709.098953	8000.116438	11.577959	-0.137368	4.816927
709.693451	8000.117330	11.582963	-0.137478	4.816925
709.795240	8000.094581	11.587968	-0.137497	4.816918
709.614287	8000.089616	11.592973	-0.137464	4.816917
709.915537	8000.100716	11.597978	-0.137520	4.816919
709.577167	8000.085860	11.602983	-0.137457	4.816916
709.382250	8000.148444	11.607987	-0.137421	4.816936
709.410386	8000.151007	11.612992	-0.137426	4.816936
709.585282	8000.094466	11.617997	-0.137458	4.816919
709.735111	8000.119064	11.623002	-0.137486	4.816925
709.276213	8000.108664	11.628007	-0.137401	4.816924
709.247690	8000.146337	11.633011	-0.137396	4.816936
709.164205	8000.168320	11.638016	-0.137380	4.816942
708.804297	8000.139361	11.643021	-0.137313	4.816936
709.135206	8000.149867	11.648026	-0.137375	4.816937
708.989441	8000.106278	11.653031	-0.137348	4.816925
708.926551	8000.217532	11.658035	-0.137336	4.816958
708.687771	8000.237070	11.663040	-0.137292	4.816965
708.902664	8000.220337	11.668045	-0.137332	4.816959
708.832602	8000.314536	11.673050	-0.137319	4.816987
709.138047	8000.204988	11.678055	-0.137376	4.816953
709.264410	8000.197451	11.683059	-0.137399	4.816951
709.213158	8000.201940	11.688064	-0.137390	4.816952
709.138081	8000.172170	11.693069	-0.137376	4.816944
709.275213	8000.231512	11.698074	-0.137401	4.816961
709.444030	8000.130401	11.703079	-0.137433	4.816930
709.441045	8000.162124	11.708083	-0.137432	4.816939
709.213910	8000.237966	11.713088	-0.137390	4.816963
709.615462	8000.184994	11.718093	-0.137465	4.816945
709.587862	8000.198328	11.723098	-0.137460	4.816949
709.150606	8000.172384	11.728103	-0.137378	4.816944
709.194470	8000.232375	11.733107	-0.137386	4.816961
709.292087	8000.233915	11.738112	-0.137405	4.816961
709.334940	8000.178470	11.743117	-0.137413	4.816945
709.746606	8000.199781	11.748122	-0.137489	4.816949
709.827862	8000.100467	11.753127	-0.137504	4.816919
709.821015	8000.127893	11.758131	-0.137503	4.816927
709.755720	8000.087688	11.763136	-0.137491	4.816916
709.655958	8000.059647	11.768141	-0.137472	4.816908
709.711962	8000.109240	11.773146	-0.137483	4.816922
709.457176	8000.121114	11.778151	-0.137435	4.816927
709.629129	8000.231832	11.783155	-0.137468	4.816959
709.407768	8000.289764	11.788160	-0.137426	4.816977
709.489505	8000.157632	11.793165	-0.137442	4.816938
709.631935	8000.185291	11.798170	-0.137468	4.816945
709.645702	8000.116682	11.803175	-0.137471	4.816925
709.778405	8000.138893	11.808179	-0.137495	4.816931
710.103956	8000.093196	11.813184	-0.137556	4.816916
709.776683	8000.096515	11.818189	-0.137495	4.816918
710.135990	8000.137120	11.823194	-0.137562	4.816929
709.834945	8000.072023	11.828199	-0.137506	4.816911
709.936906	8000.135048	11.833203	-0.137525	4.816929
710.013756	8000.111906	11.838208	-0.137539	4.816922
709.613757	8000.129963	11.843213	-0.137465	4.816929
710.122211	8000.088205	11.848218	-0.137560	4.816914
710.059668	8000.099929	11.853223	-0.137548	4.816918
709.730730	8000.204877	11.858227	-0.137487	4.816951
709.192086	8000.238752	11.863232	-0.137387	4.816963
709.426274	8000.188439	11.868237	-0.137430	4.816947
709.783672	8000.130536	11.873242	-0.137497	4.816928
709.101397	8000.212976	11.878247	-0.137370	4.816956
709.108028	8000.206730	11.883251	-0.137371	4.816954
709.316516	8000.238606	11.888256	-0.137410	4.816962
709.075058	8000.199862	11.893261	-0.137365	4.816952
708.699688	8000.322079	11.898266	-0.137295	4.816990
709.036464	8000.213025	11.903271	-0.137358	4.816956
709.557987	8000.179943	11.908275	-0.137455	4.816944
709.326731	8000.235601	11.913280	-0.137412	4.816961
709.314136	8000.183520	11.918285	-0.137410	4.816946
709.574812	8000.229983	11.923290	-0.137458	4.816959
709.493675	8000.165174	11.928295	-0.137443	4.816940
709.572932	8000.157953	11.933299	-0.137458	4.816937
709.614770	8000.182969	11.938304	-0.137466	4.816945
709.394352	8000.255741	11.943309	-0.137425	4.816967
709.490899	8000.248793	11.948314	-0.137443	4.816965
709.594831	8000.167837	11.953319	-0.137462	4.816940
709.878939	8000.136312	11.958323	-0.137515	4.816930
709.879210	8000.151143	11.963328	-0.137515	4.816934
709.560007	8000.213888	11.968333	-0.137456	4.816954
710.050930	8000.135851	11.973338	-0.137547	4.816929
710.117679	8000.094548	11.978343	-0.137560	4.816916
710.026759	8000.130180	11.983347	-0.137543	4.816927
710.172775	8000.166368	11.988352	-0.137570	4.816937
710.053331	8000.132721	11.993357	-0.137548	4.816928
709.583894	8000.229103	11.998362	-0.137460	4.816958
709.084366	8000.240298	12.003367	-0.137367	4.816964
709.322297	8000.228164	12.008371	-0.137412	4.816959
709.752562	8000.220118	12.013376	-0.137492	4.816955
709.553304	8000.190510	12.018381	-0.137455	4.816947
709.881643	8000.141679	12.023386	-0.137516	4.816931
710.056618	8000.077726	12.028391	-0.137548	4.816911
710.170358	8000.083756	12.033395	-0.137570	4.816913
709.895621	8000.106963	12.038400	-0.137519	4.816921
709.877388	8000.093971	12.043405	-0.137515	4.816917
709.648207	8000.185665	12.048410	-0.137473	4.816945
710.002840	8000.139367	12.053415	-0.137539	4.816930
710.180295	8000.145341	12.058419	-0.137572	4.816931
710.499386	8000.088953	12.063424	-0.137631	4.816913
710.221624	8000.063402	12.068429	-0.137579	4.816906
710.022070	8000.223333	12.073434	-0.137542	4.816955
709.861418	8000.166800	12.078439	-0.137512	4.816939
710.008531	8000.143706	12.083443	-0.137540	4.816931
710.261747	8000.136049	12.088448	-0.137587	4.816928
709.720122	8000.198467	12.093453	-0.137486	4.816949
709.613967	8000.275156	12.098458	-0.137467	4.816972
709.344440	8000.277267	12.103463	-0.137416	4.816974
709.928201	8000.201752	12.108467	-0.137525	4.816949
709.951934	8000.144947	12.113472	-0.137529	4.816932
709.862363	8000.139303	12.118477	-0.137513	4.816931
710.239715	8000.144190	12.123482	-0.137583	4.816930
709.831874	8000.127179	12.128487	-0.137507	4.816927
710.130945	8000.117067	12.133491	-0.137563	4.816923
710.211719	8000.125754	12.138496	-0.137578	4.816925
709.672231	8000.206207	12.143501	-0.137478	4.816951
709.794379	8000.190132	12.148506	-0.137500	4.816946
710.007407	8000.137368	12.153511	-0.137540	4.816929
710.280693	8000.128968	12.158515	-0.137591	4.816926
710.000894	8000.176450	12.163520	-0.137539	4.816941
709.417595	8000.199032	12.168525	-0.137430	4.816950
709.853396	8000.196368	12.173530	-0.137511	4.816947
709.784213	8000.174103	12.178535	-0.137499	4.816941
709.787742	8000.156159	12.183539	-0.137499	4.816936
710.055509	8000.182616	12.188544	-0.137549	4.816942
709.942525	8000.159661	12.193549	-0.137528	4.816936
710.271902	8000.143673	12.198554	-0.137589	4.816930
709.963987	8000.095410	12.203559	-0.137532	4.816917
710.383973	8000.030022	12.208563	-0.137610	4.816896
710.404510	8000.077999	12.213568	-0.137614	4.816910
710.363235	8000.061467	12.218573	-0.137607	4.816905
710.136755	8000.144733	12.223578	-0.137564	4.816931
710.513671	8000.094550	12.228583	-0.137635	4.816914
710.730593	8000.111736	12.233587	-0.137675	4.816918
710.335987	8000.130936	12.238592	-0.137602	4.816926
710.116999	8000.199495	12.243597	-0.137561	4.816947
709.952489	8000.286913	12.248602	-0.137530	4.816974
710.045350	8000.180369	12.253607	-0.137548	4.816942
709.873867	8000.209437	12.258611	-0.137516	4.816951
709.929016	8000.218780	12.263616	-0.137526	4.816954
709.910060	8000.187775	12.268621	-0.137523	4.816945
710.331198	8000.182764	12.273626	-0.137601	4.816941
710.098562	8000.168512	12.278631	-0.137558	4.816938
709.901294	8000.228942	12.283635	-0.137521	4.816957
709.954220	8000.229778	12.288640	-0.137531	4.816957
710.265542	8000.162678	12.293645	-0.137589	4.816936
709.986188	8000.322412	12.298650	-0.137537	4.816984
710.198209	8000.153151	12.303655	-0.137576	4.816933
710.200795	8000.135192	12.308659	-0.137577	4.816928
710.318184	8000.146574	12.313664	-0.137599	4.816931
710.667121	8000.095951	12.318669	-0.137664	4.816914
710.595253	8000.107528	12.323674	-0.137650	4.816918
710.229310	8000.126121	12.328679	-0.137582	4.816925
709.969754	8000.198276	12.333683	-0.137534	4.816947
710.362160	8000.168457	12.338688	-0.137607	4.816937
710.439169	8000.099784	12.343693	-0.137621	4.816916
710.536845	8000.144741	12.348698	-0.137640	4.816929
710.601142	8000.115048	12.353703	-0.137652	4.816920
710.299876	8000.143130	12.358707	-0.137596	4.816930
710.241518	8000.171863	12.363712	-0.137585	4.816938
710.662305	8000.102252	12.368717	-0.137663	4.816916
710.635608	8000.127248	12.373722	-0.137658	4.816923
710.191977	8000.156265	12.378727	-0.137576	4.816934
709.878904	8000.219106	12.383731	-0.137517	4.816954
710.164973	8000.181258	12.388736	-0.137571	4.816941
710.286612	8000.146115	12.393741	-0.137593	4.816931
710.106651	8000.247056	12.398746	-0.137560	4.816961
710.234923	8000.158012	12.403751	-0.137584	4.816934
709.821299	8000.206562	12.408755	-0.137507	4.816951
710.154672	8000.171577	12.413760	-0.137569	4.816939
710.367113	8000.121980	12.418765	-0.137608	4.816923
710.113024	8000.174103	12.423770	-0.137561	4.816940
710.125942	8000.138305	12.428775	-0.137564	4.816929
710.345219	8000.171412	12.433779	-0.137604	4.816938
710.247054	8000.211165	12.438784	-0.137586	4.816950
710.189616	8000.126609	12.443789	-0.137576	4.816925
710.288732	8000.164175	12.448794	-0.137594	4.816936
710.104786	8000.161280	12.453799	-0.137560	4.816936
709.616740	8000.200187	12.458803	-0.137469	4.816950
709.885303	8000.208655	12.463808	-0.137519	4.816951
709.837212	8000.148601	12.468813	-0.137510	4.816933
709.638968	8000.218545	12.473818	-0.137473	4.816955
710.059566	8000.202936	12.478823	-0.137552	4.816948
710.008152	8000.178832	12.483827	-0.137542	4.816941
710.534792	8000.165953	12.488832	-0.137640	4.816935
710.462747	8000.153172	12.493837	-0.137627	4.816932
710.714433	8000.178318	12.498842	-0.137674	4.816938
710.731979	8000.122474	12.503847	-0.137677	4.816921
710.690239	8000.179001	12.508851	-0.137669	4.816938
710.453233	8000.305517	12.513856	-0.137625	4.816977
710.907996	8000.184555	12.518861	-0.137710	4.816939
710.676706	8000.234918	12.523866	-0.137667	4.816955
710.888912	8000.132371	12.528871	-0.137706	4.816924
710.668263	8000.106659	12.533875	-0.137665	4.816917
710.695752	8000.114507	12.538880	-0.137670	4.816919
710.570957	8000.097719	12.543885	-0.137647	4.816915
710.441491	8000.172983	12.548890	-0.137623	4.816938
710.686202	8000.110128	12.553895	-0.137669	4.816918
710.857545	8000.110712	12.558899	-0.137701	4.816917
710.521092	8000.131887	12.563904	-0.137638	4.816925
710.218725	8000.145127	12.568909	-0.137582	4.816931
710.399652	8000.132096	12.573914	-0.137615	4.816926
710.152579	8000.155738	12.578919	-0.137569	4.816934
710.481859	8000.152457	12.583923	-0.137631	4.816931
710.563979	8000.135751	12.588928	-0.137646	4.816926
710.427141	8000.101830	12.593933	-0.137621	4.816917
710.388451	8000.170053	12.598938	-0.137613	4.816937
710.205889	8000.160825	12.603943	-0.137579	4.816935
710.446821	8000.129679	12.608947	-0.137624	4.816925
710.871057	8000.122599	12.613952	-0.137703	4.816921
710.515621	8000.088411	12.618957	-0.137637	4.816912
710.455218	8000.192295	12.623962	-0.137626	4.816943
710.100714	8000.146473	12.628967	-0.137560	4.816931
710.076709	8000.210691	12.633971	-0.137556	4.816951
710.111068	8000.216530	12.638976	-0.137562	4.816952
710.324772	8000.105535	12.643981	-0.137602	4.816918
710.572169	8000.143321	12.648986	-0.137648	4.816928
710.229508	8000.156985	12.653991	-0.137584	4.816934
710.259987	8000.178646	12.658995	-0.137590	4.816940
710.595774	8000.142641	12.664000	-0.137652	4.816928
710.352607	8000.128223	12.669005	-0.137607	4.816925
709.997163	8000.200986	12.674010	-0.137541	4.816948
709.823655	8000.209903	12.679015	-0.137509	4.816951
710.134691	8000.119503	12.684019	-0.137567	4.816923
710.258732	8000.161698	12.689024	-0.137590	4.816935
710.532162	8000.112003	12.694029	-0.137641	4.816919
710.398122	8000.161781	12.699034	-0.137616	4.816935
710.140930	8000.187381	12.704039	-0.137568	4.816943
710.503307	8000.144382	12.709043	-0.137635	4.816929
710.121315	8000.242140	12.714048	-0.137564	4.816960
710.546661	8000.172602	12.719053	-0.137644	4.816937
710.722240	8000.160546	12.724058	-0.137676	4.816933
710.389023	8000.155298	12.729063	-0.137614	4.816933
710.506416	8000.180446	12.734067	-0.137636	4.816940
710.539489	8000.194736	12.739072	-0.137642	4.816944
710.802335	8000.130049	12.744077	-0.137691	4.816923
710.786574	8000.159453	12.749082	-0.137688	4.816932
710.962331	8000.096571	12.754087	-0.137721	4.816913
711.027865	8000.117726	12.759091	-0.137733	4.816919
710.739751	8000.175665	12.764096	-0.137680	4.816937
710.978732	8000.118015	12.769101	-0.137724	4.816919
711.095080	8000.112439	12.774106	-0.137746	4.816917
710.941371	8000.078251	12.779111	-0.137717	4.816907
710.992711	8000.127773	12.784115	-0.137727	4.816922
710.968674	8000.126338	12.789120	-0.137722	4.816921
710.800075	8000.109917	12.794125	-0.137691	4.816917
710.749688	8000.136658	12.799130	-0.137682	4.816926
710.915840	8000.108569	12.804135	-0.137713	4.816916
710.712180	8000.154073	12.809139	-0.137675	4.816931
710.451889	8000.181742	12.814144	-0.137626	4.816940
710.556637	8000.121978	12.819149	-0.137646	4.816922
710.770817	8000.159240	12.824154	-0.137686	4.816932
710.599907	8000.189376	12.829159	-0.137654	4.816942
710.548564	8000.174804	12.834163	-0.137645	4.816938
710.904281	8000.163468	12.839168	-0.137711	4.816933
710.486392	8000.143120	12.844173	-0.137633	4.816929
710.609252	8000.148235	12.849178	-0.137656	4.816930
710.531674	8000.219022	12.854183	-0.137642	4.816951
710.620147	8000.138881	12.859187	-0.137658	4.816927
710.338544	8000.207512	12.864192	-0.137606	4.816948
710.541998	8000.120712	12.869197	-0.137643	4.816922
710.781690	8000.159435	12.874202	-0.137688	4.816932
710.259806	8000.225339	12.879207	-0.137591	4.816954
709.999237	8000.212765	12.884211	-0.137543	4.816951
710.870294	8000.195783	12.889216	-0.137705	4.816942
710.513285	8000.146744	12.894221	-0.137638	4.816930
710.203334	8000.215988	12.899226	-0.137581	4.816951
710.794786	8000.143772	12.904231	-0.137691	4.816927
710.796209	8000.143796	12.909235	-0.137691	4.816927
711.004882	8000.122731	12.914240	-0.137730	4.816920
710.888495	8000.159021	12.919245	-0.137708	4.816931
710.838617	8000.190006	12.924250	-0.137699	4.816941
710.675273	8000.213907	12.929255	-0.137669	4.816949
710.546665	8000.179056	12.934259	-0.137645	4.816939
710.345411	8000.225657	12.939264	-0.137607	4.816954
710.320510	8000.231621	12.944269	-0.137603	4.816956
710.193532	8000.269862	12.949274	-0.137579	4.816967
710.412223	8000.260603	12.954279	-0.137620	4.816964
710.648071	8000.184902	12.959283	-0.137664	4.816940
710.802260	8000.206394	12.964288	-0.137693	4.816946
710.540303	8000.201210	12.969293	-0.137644	4.816946
710.940139	8000.204336	12.974298	-0.137718	4.816945
710.182908	8000.324772	12.979303	-0.137577	4.816984
710.268124	8000.246698	12.984307	-0.137593	4.816960
710.515056	8000.252709	12.989312	-0.137639	4.816961
710.376404	8000.243114	12.994317	-0.137613	4.816959
710.489324	8000.243837	12.999322	-0.137634	4.816958
710.306984	8000.275911	13.004327	-0.137601	4.816969
710.145322	8000.238422	13.009331	-0.137570	4.816958
710.423353	8000.206801	13.014336	-0.137622	4.816948
710.443181	8000.232530	13.019341	-0.137626	4.816955
711.056984	8000.167021	13.024346	-0.137740	4.816933
710.808832	8000.154641	13.029351	-0.137694	4.816931
710.599807	8000.146055	13.034355	-0.137655	4.816929
710.852934	8000.178637	13.039360	-0.137702	4.816937
710.763516	8000.159229	13.044365	-0.137686	4.816932
710.919144	8000.128856	13.049370	-0.137715	4.816922
710.868518	8000.149240	13.054375	-0.137705	4.816929
710.977348	8000.150957	13.059379	-0.137726	4.816929
711.054337	8000.162762	13.064384	-0.137740	4.816932
710.914610	8000.130912	13.069389	-0.137714	4.816923
710.981260	8000.162674	13.074394	-0.137726	4.816932
710.950461	8000.177016	13.079399	-0.137721	4.816936
710.712553	8000.172210	13.084403	-0.137676	4.816936
710.942253	8000.236192	13.089408	-0.137719	4.816954
710.999169	8000.144964	13.094413	-0.137730	4.816927
710.824071	8000.203625	13.099418	-0.137697	4.816945
710.733587	8000.174669	13.104423	-0.137680	4.816937
711.113878	8000.118187	13.109427	-0.137751	4.816918
710.783765	8000.139461	13.114432	-0.137690	4.816926
710.933229	8000.118522	13.119437	-0.137718	4.816919
711.219588	8000.147392	13.124442	-0.137771	4.816926
711.083095	8000.134654	13.129447	-0.137746	4.816923
710.960175	8000.121071	13.134451	-0.137723	4.816920
710.760466	8000.220643	13.139456	-0.137686	4.816950
711.146306	8000.135658	13.144461	-0.137758	4.816923
710.558600	8000.204760	13.149466	-0.137648	4.816946
710.798827	8000.240316	13.154471	-0.137693	4.816956
711.086778	8000.188732	13.159475	-0.137747	4.816939
711.025448	8000.198358	13.164480	-0.137735	4.816942
711.096721	8000.137006	13.169485	-0.137748	4.816924
711.126067	8000.168180	13.174490	-0.137754	4.816933
710.520651	8000.192528	13.179495	-0.137641	4.816943
710.775022	8000.154181	13.184499	-0.137689	4.816931
710.603572	8000.188544	13.189504	-0.137657	4.816941
710.440280	8000.197622	13.194509	-0.137626	4.816945
710.344573	8000.223649	13.199514	-0.137609	4.816953
710.772584	8000.171095	13.204519	-0.137688	4.816936
710.663297	8000.229734	13.209523	-0.137668	4.816953
710.613677	8000.246957	13.214528	-0.137659	4.816959
710.373827	8000.272830	13.219533	-0.137614	4.816967
710.623033	8000.228048	13.224538	-0.137661	4.816953
710.451840	8000.309008	13.229543	-0.137629	4.816978
710.804450	8000.197026	13.234547	-0.137694	4.816943
710.677063	8000.307268	13.239552	-0.137671	4.816976
710.806791	8000.221423	13.244557	-0.137695	4.816950
710.365533	8000.275890	13.249562	-0.137613	4.816968
710.372521	8000.272825	13.254567	-0.137614	4.816967
710.997122	8000.160893	13.259571	-0.137730	4.816931
710.970036	8000.207062	13.264576	-0.137725	4.816945
710.690436	8000.167713	13.269581	-0.137673	4.816935
710.519743	8000.225385	13.274586	-0.137642	4.816953
710.931858	8000.223410	13.279591	-0.137718	4.816950
710.876215	8000.180178	13.284595	-0.137708	4.816938
710.841839	8000.213525	13.289600	-0.137702	4.816948
710.985294	8000.142721	13.294605	-0.137728	4.816926
710.747399	8000.194039	13.299610	-0.137684	4.816942
710.835504	8000.218727	13.304615	-0.137701	4.816949
711.181873	8000.138414	13.309619	-0.137765	4.816924
711.021942	8000.160251	13.314624	-0.137735	4.816931
711.237044	8000.113873	13.319629	-0.137775	4.816916
711.386146	8000.136345	13.324634	-0.137803	4.816922
711.191254	8000.161867	13.329639	-0.137767	4.816931
710.881989	8000.140053	13.334643	-0.137709	4.816926
711.019976	8000.164468	13.339648	-0.137735	4.816932
711.106864	8000.147837	13.344653	-0.137751	4.816927
711.068902	8000.172656	13.349658	-0.137744	4.816935
710.891920	8000.185753	13.354663	-0.137711	4.816939
711.011382	8000.173872	13.359667	-0.137734	4.816935
710.998514	8000.229795	13.364672	-0.137731	4.816952
711.055644	8000.167162	13.369677	-0.137742	4.816933
711.687781	8000.132652	13.374682	-0.137860	4.816920
711.285410	8000.154903	13.379687	-0.137785	4.816928
711.425671	8000.113700	13.384691	-0.137811	4.816916
711.803367	8000.124950	13.389696	-0.137881	4.816917
711.881182	8000.080644	13.394701	-0.137896	4.816904
711.695549	8000.125373	13.399706	-0.137861	4.816918
711.237677	8000.150986	13.404711	-0.137776	4.816927
711.299154	8000.133955	13.409715	-0.137787	4.816922
711.601226	8000.119658	13.414720	-0.137844	4.816916
711.189775	8000.116352	13.419725	-0.137767	4.816917
711.026499	8000.165669	13.424730	-0.137737	4.816933
711.491134	8000.128519	13.429735	-0.137823	4.816920
711.379823	8000.106647	13.434739	-0.137803	4.816914
711.641412	8000.146777	13.439744	-0.137851	4.816924
711.455825	8000.133264	13.444749	-0.137817	4.816921
711.560408	8000.150799	13.449754	-0.137836	4.816926
711.359811	8000.129638	13.454759	-0.137799	4.816921
711.645529	8000.117200	13.459763	-0.137852	4.816916
711.508573	8000.146812	13.464768	-0.137827	4.816925
711.626833	8000.119028	13.469773	-0.137849	4.816916
711.837595	8000.129765	13.474778	-0.137888	4.816918
711.606468	8000.133537	13.479783	-0.137845	4.816921
711.387751	8000.139623	13.484787	-0.137804	4.816923
711.417463	8000.155978	13.489792	-0.137810	4.816928
711.580837	8000.113020	13.494797	-0.137840	4.816915
711.563974	8000.112757	13.499802	-0.137837	4.816915
711.667564	8000.099567	13.504807	-0.137857	4.816910
711.305105	8000.125625	13.509811	-0.137789	4.816920
711.276448	8000.171769	13.514816	-0.137784	4.816933
711.366527	8000.126597	13.519821	-0.137801	4.816920
711.796961	8000.130207	13.524826	-0.137881	4.816919
711.776920	8000.124599	13.529831	-0.137877	4.816917
711.588992	8000.121639	13.534835	-0.137842	4.816917
711.538284	8000.165318	13.539840	-0.137833	4.816930
711.556826	8000.094663	13.544845	-0.137836	4.816909
711.555746	8000.135947	13.549850	-0.137836	4.816921
711.288385	8000.147620	13.554855	-0.137786	4.816926
711.450255	8000.115228	13.559859	-0.137816	4.816916
711.832114	8000.164667	13.564864	-0.137888	4.816929
711.141867	8000.144259	13.569869	-0.137759	4.816926
711.449284	8000.144871	13.574874	-0.137816	4.816925
711.465846	8000.175844	13.579879	-0.137819	4.816934
711.400956	8000.139878	13.584883	-0.137807	4.816923
711.466643	8000.147269	13.589888	-0.137820	4.816925
711.364546	8000.112835	13.594893	-0.137801	4.816916
711.654004	8000.139638	13.599898	-0.137855	4.816922
711.660646	8000.115389	13.604903	-0.137856	4.816915
711.299908	8000.113941	13.609907	-0.137789	4.816916
711.592354	8000.170441	13.614912	-0.137843	4.816931
711.484055	8000.141204	13.619917	-0.137823	4.816923
711.681022	8000.141134	13.624922	-0.137860	4.816922
711.742869	8000.123050	13.629927	-0.137871	4.816917
711.466800	8000.137762	13.634931	-0.137820	4.816922
711.333889	8000.149436	13.639936	-0.137795	4.816926
711.854757	8000.123762	13.644941	-0.137892	4.816916
711.657473	8000.129126	13.649946	-0.137856	4.816919
711.271370	8000.144222	13.654951	-0.137784	4.816925
710.962262	8000.152060	13.659955	-0.137726	4.816929
710.884932	8000.227087	13.664960	-0.137712	4.816951
710.732888	8000.181278	13.669965	-0.137684	4.816939
710.691275	8000.231453	13.674970	-0.137676	4.816954
711.070626	8000.159072	13.679975	-0.137746	4.816931
711.262372	8000.153625	13.684979	-0.137782	4.816928
711.332589	8000.199210	13.689984	-0.137795	4.816941
710.780244	8000.210627	13.694989	-0.137692	4.816947
710.725386	8000.272242	13.699994	-0.137682	4.816965
710.758508	8000.287591	13.704999	-0.137689	4.816970
710.724069	8000.248929	13.710003	-0.137682	4.816959
710.818413	8000.272656	13.715008	-0.137700	4.816965
710.878710	8000.233369	13.720013	-0.137711	4.816953
710.578163	8000.280523	13.725018	-0.137655	4.816969
711.000564	8000.243766	13.730023	-0.137734	4.816956
711.060452	8000.186470	13.735027	-0.137745	4.816939
711.176635	8000.153358	13.740032	-0.137767	4.816928
710.824980	8000.161585	13.745037	-0.137701	4.816932
710.867211	8000.194021	13.750042	-0.137709	4.816942
710.837847	8000.262392	13.755047	-0.137704	4.816962
710.281336	8000.281156	13.760051	-0.137600	4.816970
710.691356	8000.308799	13.765056	-0.137676	4.816976
711.038140	8000.214726	13.770061	-0.137741	4.816947
710.765106	8000.215720	13.775066	-0.137690	4.816949
711.147846	8000.207989	13.780071	-0.137761	4.816945
711.340100	8000.177135	13.785075	-0.137797	4.816935
711.081583	8000.192124	13.790080	-0.137749	4.816940
710.769104	8000.220029	13.795085	-0.137691	4.816950
711.026964	8000.217741	13.800090	-0.137739	4.816948
710.662435	8000.311539	13.805095	-0.137671	4.816977
710.075586	8000.375359	13.810099	-0.137562	4.816999
710.322353	8000.368661	13.815104	-0.137608	4.816996
710.522773	8000.310404	13.820109	-0.137645	4.816978
709.951553	8000.370235	13.825114	-0.137539	4.816998
710.466675	8000.309524	13.830119	-0.137635	4.816978
710.497624	8000.271893	13.835123	-0.137641	4.816966
710.498248	8000.335441	13.840128	-0.137641	4.816985
710.560055	8000.253820	13.845133	-0.137652	4.816961
710.538442	8000.323372	13.850138	-0.137648	4.816981
710.416303	8000.386044	13.855143	-0.137626	4.817000
710.309509	8000.361067	13.860147	-0.137606	4.816994
710.110908	8000.383354	13.865152	-0.137569	4.817001
710.660752	8000.282951	13.870157	-0.137671	4.816969
710.604029	8000.293708	13.875162	-0.137661	4.816972
710.930541	8000.332743	13.880167	-0.137722	4.816982
711.497227	8000.180717	13.885171	-0.137827	4.816935
710.994436	8000.330578	13.890176	-0.137734	4.816981
711.179202	8000.193712	13.895181	-0.137768	4.816940
710.683463	8000.274852	13.900186	-0.137676	4.816966
710.463569	8000.332807	13.905191	-0.137635	4.816985
710.369013	8000.314376	13.910195	-0.137617	4.816980
710.647044	8000.297582	13.915200	-0.137669	4.816973
710.258553	8000.335937	13.920205	-0.137597	4.816986
710.494363	8000.316359	13.925210	-0.137641	4.816980
710.583178	8000.317761	13.930215	-0.137657	4.816980
710.493645	8000.316352	13.935219	-0.137641	4.816980
710.567859	8000.357764	13.940224	-0.137654	4.816991
710.304587	8000.323967	13.945229	-0.137605	4.816983
710.614188	8000.269548	13.950234	-0.137663	4.816965
710.833648	8000.310072	13.955239	-0.137704	4.816976
710.968072	8000.199945	13.960243	-0.137729	4.816943
710.873563	8000.242934	13.965248	-0.137711	4.816956
710.411996	8000.321436	13.970253	-0.137626	4.816981
711.029977	8000.214694	13.975258	-0.137741	4.816947
711.173092	8000.226483	13.980263	-0.137767	4.816950
710.919415	8000.295554	13.985267	-0.137720	4.816971
711.206250	8000.233364	13.990272	-0.137773	4.816952
710.778350	8000.303924	13.995277	-0.137694	4.816975
710.559492	8000.350248	14.000282	-0.137653	4.816989
710.811051	8000.291737	14.005287	-0.137700	4.816971
710.980384	8000.267935	14.010291	-0.137732	4.816963
711.085855	8000.316193	14.015296	-0.137751	4.816977
710.961626	8000.317414	14.020301	-0.137728	4.816978
711.038133	8000.227553	14.025306	-0.137742	4.816951
710.291570	8000.398986	14.030311	-0.137603	4.817005
710.589571	8000.305204	14.035315	-0.137659	4.816976
710.444535	8000.427875	14.040320	-0.137632	4.817013
710.712241	8000.321967	14.045325	-0.137682	4.816980
710.495428	8000.293138	14.050330	-0.137641	4.816973
710.306119	8000.400286	14.055335	-0.137606	4.817005
710.422386	8000.327995	14.060339	-0.137628	4.816983
710.338365	8000.413506	14.065344	-0.137612	4.817009
710.593475	8000.328578	14.070349	-0.137660	4.816983
710.854825	8000.287165	14.075354	-0.137709	4.816969
710.645716	8000.332583	14.080359	-0.137670	4.816984
710.575644	8000.339953	14.085363	-0.137657	4.816986
710.488439	8000.361877	14.090368	-0.137640	4.816993
710.684495	8000.292962	14.095373	-0.137677	4.816972
710.926982	8000.206776	14.100378	-0.137722	4.816945
710.856126	8000.288259	14.105383	-0.137709	4.816970
710.741683	8000.277986	14.110387	-0.137688	4.816967
710.724013	8000.298889	14.115392	-0.137684	4.816973
711.078359	8000.274826	14.120397	-0.137750	4.816965
711.307719	8000.226555	14.125402	-0.137793	4.816949
711.526956	8000.196127	14.130407	-0.137834	4.816939
711.006591	8000.247228	14.135411	-0.137737	4.816957
711.163736	8000.262415	14.140416	-0.137766	4.816961
711.005282	8000.236623	14.145421	-0.137737	4.816954
711.071632	8000.264144	14.150426	-0.137749	4.816961
711.132467	8000.295815	14.155431	-0.137761	4.816970
711.294962	8000.174482	14.160435	-0.137791	4.816934
710.920479	8000.192938	14.165440	-0.137721	4.816941
710.992225	8000.176069	14.170445	-0.137735	4.816936
711.513803	8000.127109	14.175450	-0.137832	4.816919
711.744648	8000.163577	14.180455	-0.137875	4.816929
711.188003	8000.190810	14.185459	-0.137771	4.816939
711.404848	8000.245060	14.190464	-0.137812	4.816954
711.483916	8000.187007	14.195469	-0.137826	4.816937
711.627273	8000.159619	14.200474	-0.137853	4.816928
711.766712	8000.173468	14.205479	-0.137879	4.816931
711.493195	8000.177630	14.210483	-0.137828	4.816934
711.620943	8000.208238	14.215488	-0.137852	4.816942
711.570618	8000.172501	14.220493	-0.137843	4.816932
712.153933	8000.149931	14.225498	-0.137951	4.816923
712.116947	8000.150409	14.230503	-0.137944	4.816923
711.730734	8000.136910	14.235507	-0.137872	4.816921
711.429043	8000.226404	14.240512	-0.137816	4.816949
711.542163	8000.169947	14.245517	-0.137837	4.816931
711.267550	8000.202684	14.250522	-0.137786	4.816942
711.520130	8000.197137	14.255527	-0.137833	4.816940
711.513110	8000.228797	14.260531	-0.137832	4.816949
711.277748	8000.245209	14.265536	-0.137788	4.816955
711.050424	8000.270220	14.270541	-0.137746	4.816963
711.204909	8000.221828	14.275546	-0.137775	4.816948
711.543990	8000.202820	14.280551	-0.137838	4.816941
711.616846	8000.153141	14.285555	-0.137852	4.816926
711.131755	8000.246097	14.290560	-0.137761	4.816956
711.132852	8000.249293	14.295565	-0.137762	4.816957
711.318863	8000.205634	14.300570	-0.137796	4.816943
711.366270	8000.241329	14.305575	-0.137805	4.816953
711.924627	8000.133648	14.310579	-0.137909	4.816919
712.078558	8000.183731	14.315584	-0.137938	4.816933
711.625608	8000.210479	14.320589	-0.137853	4.816943
711.411659	8000.231464	14.325594	-0.137814	4.816950
711.862252	8000.194094	14.330599	-0.137897	4.816937
711.428960	8000.173499	14.335603	-0.137817	4.816933
711.648438	8000.179079	14.340608	-0.137858	4.816934
711.695444	8000.224299	14.345613	-0.137867	4.816947
711.795698	8000.176111	14.350618	-0.137885	4.816932
712.143297	8000.148765	14.355623	-0.137950	4.816922
712.322913	8000.106064	14.360627	-0.137983	4.816909
712.568828	8000.133242	14.365632	-0.138029	4.816916
712.348324	8000.081054	14.370637	-0.137988	4.816901
712.297099	8000.122608	14.375642	-0.137979	4.816914
712.696175	8000.118313	14.380647	-0.138053	4.816911
712.239403	8000.114290	14.385651	-0.137968	4.816912
712.222122	8000.143671	14.390656	-0.137965	4.816921
712.328070	8000.130518	14.395661	-0.137985	4.816916
712.131954	8000.146490	14.400666	-0.137948	4.816922
712.270202	8000.126434	14.405671	-0.137974	4.816915
711.866314	8000.132776	14.410675	-0.137899	4.816919
711.924170	8000.177108	14.415680	-0.137909	4.816932
711.880517	8000.136182	14.420685	-0.137901	4.816920
711.998004	8000.149685	14.425690	-0.137923	4.816923
712.106221	8000.191634	14.430695	-0.137943	4.816935
711.855242	8000.133672	14.435699	-0.137897	4.816919
711.940949	8000.155146	14.440704	-0.137913	4.816925
711.707534	8000.243598	14.445709	-0.137869	4.816952
711.807042	8000.154099	14.450714	-0.137888	4.816926
711.968341	8000.165115	14.455719	-0.137918	4.816928
711.972872	8000.115418	14.460723	-0.137919	4.816913
712.216342	8000.122436	14.465728	-0.137964	4.816914
712.126726	7999.097041	14.470733	-0.137947	4.816612

712.299669	7996.050418	14.475738	-0.137977	4.815713
712.618750	7990.547882	14.480743	-0.138033	4.814089
712.293954	7983.989834	14.485747	-0.137968	4.812155
712.197123	7976.687199	14.490752	-0.137945	4.810000
712.298029	7969.117096	14.495757	-0.137959	4.807764
711.974867	7961.313893	14.500762	-0.137894	4.805460
711.734685	7953.470372	14.505767	-0.137844	4.803143
711.652172	7945.520083	14.510771	-0.137824	4.800792
711.365111	7937.537060	14.515776	-0.137765	4.798431
711.242662	7929.529819	14.520781	-0.137737	4.796061
711.529375	7921.493268	14.525786	-0.137785	4.793680
711.923456	7913.514741	14.530791	-0.137853	4.791314
711.556587	7905.459232	14.535795	-0.137780	4.788927
711.627007	7897.527334	14.540800	-0.137788	4.786574
711.606874	7889.479288	14.545805	-0.137779	4.784186
711.568522	7881.486552	14.550810	-0.137767	4.781813
711.611222	7873.510392	14.555815	-0.137769	4.779443
711.678600	7865.504883	14.560819	-0.137777	4.777063
711.622236	7857.478733	14.565824	-0.137761	4.774677
711.592412	7849.489469	14.570829	-0.137750	4.772300
711.697260	7841.407242	14.575834	-0.137765	4.769894
711.574290	7833.503515	14.580839	-0.137737	4.767541
711.149329	7825.473517	14.585843	-0.137652	4.765150
711.276802	7817.453975	14.590848	-0.137671	4.762758
711.345406	7809.472299	14.595853	-0.137678	4.760378
711.396508	7801.460937	14.600858	-0.137683	4.757987
711.320806	7793.465819	14.605863	-0.137663	4.755600
711.276262	7785.445825	14.610867	-0.137650	4.753205
711.382473	7777.468012	14.615872	-0.137665	4.750820
711.236138	7769.398706	14.620877	-0.137632	4.748408
711.169840	7761.381312	14.625882	-0.137615	4.746009
711.281203	7753.413536	14.630887	-0.137630	4.743624
710.899319	7745.456479	14.635891	-0.137554	4.741242
710.915150	7737.432299	14.640896	-0.137552	4.738838
710.898336	7729.483736	14.645901	-0.137543	4.736455
710.755958	7721.376758	14.650906	-0.137512	4.734024
710.553054	7713.481501	14.655911	-0.137469	4.731656
710.614168	7705.349286	14.660915	-0.137475	4.729214
710.782867	7697.437246	14.665920	-0.137501	4.726837
710.680023	7689.352427	14.670925	-0.137477	4.724407
710.637759	7681.444609	14.675930	-0.137464	4.722029
710.620769	7673.471484	14.680935	-0.137455	4.719631
710.526456	7665.434438	14.685939	-0.137433	4.717212
710.266251	7657.428310	14.690944	-0.137379	4.714801
710.211824	7649.417515	14.695949	-0.137364	4.712388
710.191398	7641.333442	14.700954	-0.137355	4.709951
710.572700	7633.368077	14.705959	-0.137420	4.707547
710.478122	7625.316599	14.710963	-0.137398	4.705118
710.405870	7617.398687	14.715968	-0.137379	4.702727
709.991360	7609.451699	14.720973	-0.137297	4.700327
709.570533	7601.483083	14.725978	-0.137213	4.697920
709.908966	7593.460216	14.730983	-0.137271	4.695493
709.466947	7585.423539	14.735987	-0.137183	4.693062
709.835382	7577.377082	14.740992	-0.137247	4.690626
709.778776	7569.390138	14.745997	-0.137231	4.688207
710.019232	7561.351177	14.751002	-0.137271	4.685771
709.854461	7553.384335	14.756007	-0.137235	4.683355
709.431364	7545.420462	14.761011	-0.137151	4.680940
709.600910	7537.416232	14.766016	-0.137177	4.678511
709.359247	7529.442084	14.771021	-0.137127	4.676089
709.411584	7521.392219	14.776026	-0.137132	4.673644
709.561920	7513.337698	14.781031	-0.137154	4.671195
709.351728	7505.323981	14.786035	-0.137110	4.668758
709.242000	7497.379511	14.791040	-0.137084	4.666341
709.376728	7489.323155	14.796045	-0.137104	4.663888
709.408021	7481.387476	14.801050	-0.137105	4.661470
709.229377	7473.342642	14.806055	-0.137067	4.659019
708.990384	7465.383839	14.811059	-0.137017	4.656592
709.262055	7457.348748	14.816064	-0.137062	4.654140
709.022543	7449.403499	14.821069	-0.137012	4.651715
709.413642	7441.318744	14.826074	-0.137080	4.649246
709.563894	7433.347978	14.831079	-0.137103	4.646810
709.640238	7425.250540	14.836083	-0.137112	4.644334
709.417008	7417.414046	14.841088	-0.137065	4.641937
709.238135	7409.374738	14.846093	-0.137027	4.639477
709.266755	7401.409329	14.851098	-0.137027	4.637037
709.288552	7393.357437	14.856103	-0.137026	4.634570
709.011501	7385.389009	14.861107	-0.136969	4.632128
709.427106	7377.338824	14.866112	-0.137041	4.629658
709.161389	7369.350472	14.871117	-0.136986	4.627207
708.866043	7361.324781	14.876122	-0.136926	4.624743
709.073788	7353.394941	14.881127	-0.136960	4.622307
708.889595	7345.348438	14.886131	-0.136920	4.619833
708.963810	7337.365094	14.891136	-0.136929	4.617378
708.896193	7329.290706	14.896141	-0.136911	4.614894
708.907809	7321.333174	14.901146	-0.136908	4.612444
708.874306	7313.347491	14.906151	-0.136897	4.609984
708.435187	7305.350354	14.911155	-0.136810	4.607519
708.597411	7297.327516	14.916160	-0.136835	4.605046
708.541520	7289.360862	14.921165	-0.136819	4.602588
708.664186	7281.322354	14.926170	-0.136837	4.600106
708.665654	7273.344968	14.931175	-0.136832	4.597642
708.552356	7265.342819	14.936179	-0.136806	4.595169
708.628507	7257.330459	14.941184	-0.136815	4.592692
708.224037	7249.314527	14.946189	-0.136734	4.590212
708.716218	7241.242185	14.951194	-0.136821	4.587714
708.618927	7233.247318	14.956199	-0.136797	4.585238
708.099854	7225.309492	14.961203	-0.136695	4.582778
708.250291	7217.315548	14.966208	-0.136718	4.580299
708.285967	7209.340367	14.971213	-0.136720	4.577825
708.351878	7201.259767	14.976218	-0.136727	4.575317
708.140588	7193.320338	14.981223	-0.136682	4.572852
708.035638	7185.253257	14.986227	-0.136658	4.570345
708.299714	7177.232249	14.991232	-0.136701	4.567852
707.945530	7169.265441	14.996237	-0.136630	4.565373
708.089233	7161.234602	15.001242	-0.136652	4.562874
708.115664	7153.265815	15.006247	-0.136652	4.560393
708.197165	7145.251999	15.011251	-0.136662	4.557896
708.086872	7137.259574	15.016256	-0.136636	4.555404
708.142995	7129.295687	15.021261	-0.136641	4.552921
708.044317	7121.277995	15.026266	-0.136618	4.550418
707.832274	7113.284412	15.031271	-0.136573	4.547922
707.919678	7105.245555	15.036275	-0.136584	4.545411
708.067342	7097.265657	15.041280	-0.136606	4.542916
707.841499	7089.262546	15.046285	-0.136559	4.540413
707.666865	7081.269592	15.051290	-0.136521	4.537911
707.755332	7073.226505	15.056295	-0.136533	4.535393
707.588707	7065.235468	15.061299	-0.136496	4.532889
707.385880	7057.183465	15.066304	-0.136453	4.530365
707.695232	7049.205900	15.071309	-0.136506	4.527863
707.617591	7041.195776	15.076314	-0.136486	4.525350
707.444690	7033.261459	15.081319	-0.136449	4.522858
707.477095	7025.187887	15.086323	-0.136450	4.520322
707.451806	7017.220592	15.091328	-0.136440	4.517817
707.508141	7009.256058	15.096333	-0.136445	4.515312
707.195566	7001.242548	15.101338	-0.136382	4.512790
707.125645	6993.257303	15.106343	-0.136364	4.510275
707.138223	6985.174757	15.111347	-0.136361	4.507729
707.185338	6977.149935	15.116352	-0.136364	4.505199
707.047399	6969.211491	15.121357	-0.136333	4.502695
706.930289	6961.160621	15.126362	-0.136306	4.500154
706.846370	6953.222763	15.131367	-0.136286	4.497648
707.128296	6945.116812	15.136371	-0.136333	4.495088
706.989858	6937.171676	15.141376	-0.136302	4.492576
706.888910	6929.143822	15.146381	-0.136278	4.490036
706.630511	6921.145880	15.151386	-0.136225	4.487504
706.987933	6913.146965	15.156391	-0.136286	4.484973
706.815458	6905.210412	15.161395	-0.136249	4.482458
706.990977	6897.146542	15.166400	-0.136276	4.479902
706.748941	6889.204095	15.171405	-0.136226	4.477382
706.546276	6881.165460	15.176410	-0.136183	4.474830
706.475521	6873.164362	15.181415	-0.136165	4.472289
706.684994	6865.084957	15.186419	-0.136198	4.469723
706.545409	6857.138026	15.191424	-0.136167	4.467196
706.266561	6849.159093	15.196429	-0.136110	4.464657
706.187712	6841.164678	15.201434	-0.136090	4.462112
706.399138	6833.171195	15.206439	-0.136125	4.459567
705.950411	6825.179895	15.211443	-0.136036	4.457019
706.380355	6817.104569	15.216448	-0.136111	4.454446
706.071013	6809.200061	15.221453	-0.136048	4.451923
706.151136	6801.071019	15.226458	-0.136058	4.449329
706.038613	6793.146721	15.231463	-0.136031	4.446797
705.585262	6785.129140	15.236467	-0.135942	4.444233
705.953470	6777.162464	15.241472	-0.136005	4.441688
705.812631	6769.124520	15.246477	-0.135974	4.439115
705.438643	6761.157054	15.251482	-0.135899	4.436563
705.783074	6753.097128	15.256487	-0.135958	4.433983
705.757063	6745.111513	15.261491	-0.135948	4.431424
705.556938	6737.065981	15.266496	-0.135905	4.428843
705.704920	6729.085118	15.271501	-0.135928	4.426283
705.613742	6721.080415	15.276506	-0.135906	4.423712
705.217692	6713.173567	15.281511	-0.135827	4.421170
705.153251	6705.074917	15.286515	-0.135810	4.418567
705.296858	6697.086444	15.291520	-0.135831	4.415999
705.401353	6689.045010	15.296525	-0.135845	4.413411
705.410743	6681.004964	15.301530	-0.135842	4.410823
705.507508	6673.061198	15.306535	-0.135855	4.408264
705.378592	6665.059952	15.311539	-0.135826	4.405684
705.312371	6657.080776	15.316544	-0.135808	4.403110
705.103284	6649.080702	15.321549	-0.135764	4.400527
704.986844	6641.078015	15.326554	-0.135737	4.397942
704.561951	6633.118327	15.331559	-0.135653	4.395367
704.740375	6625.077506	15.336563	-0.135681	4.392768
704.741120	6617.052278	15.341568	-0.135676	4.390172
704.726623	6609.070648	15.346573	-0.135668	4.387588
704.919120	6601.006114	15.351578	-0.135698	4.384977
704.857374	6593.095469	15.356583	-0.135682	4.382413
704.654591	6585.045824	15.361587	-0.135639	4.379802
704.647971	6577.104138	15.366592	-0.135633	4.377225
704.773940	6569.050214	15.371597	-0.135651	4.374611
704.074712	6561.101501	15.376602	-0.135515	4.372024
704.337433	6553.033446	15.381607	-0.135559	4.369403
704.035128	6545.064722	15.386611	-0.135498	4.366810
704.130330	6536.983646	15.391616	-0.135510	4.364180
703.848826	6529.179488	15.396621	-0.135453	4.361637
703.867810	6521.048245	15.401626	-0.135451	4.358988
704.018603	6513.117411	15.406631	-0.135474	4.356403
703.688873	6505.094946	15.411635	-0.135407	4.353784
703.807154	6497.051868	15.416640	-0.135424	4.351159
704.129122	6489.002634	15.421645	-0.135479	4.348532
704.129408	6480.988840	15.426650	-0.135474	4.345913
704.391890	6472.974273	15.431655	-0.135517	4.343294
703.896391	6465.052349	15.436659	-0.135420	4.340698
703.982169	6457.074088	15.441664	-0.135431	4.338087
703.758658	6449.108357	15.446669	-0.135384	4.335476
703.292607	6441.141478	15.451674	-0.135292	4.332861
703.449310	6433.123803	15.456679	-0.135316	4.330232
703.584039	6425.081958	15.461683	-0.135336	4.327593
703.520649	6417.072289	15.466688	-0.135319	4.324963
703.329502	6409.111302	15.471693	-0.135278	4.322345
702.663778	6401.186143	15.476698	-0.135149	4.319734
703.136556	6393.163580	15.481703	-0.135232	4.317098
702.941989	6385.116888	15.486707	-0.135190	4.314448
703.059008	6377.135099	15.491712	-0.135207	4.311819
702.732508	6369.117622	15.496717	-0.135141	4.309174
702.682646	6361.120298	15.501722	-0.135127	4.306536
702.943445	6353.047527	15.506727	-0.135170	4.303874
702.767357	6345.110395	15.511731	-0.135132	4.301251
702.945754	6337.032464	15.516736	-0.135160	4.298583
703.023347	6329.072437	15.521741	-0.135169	4.295952
702.996479	6321.032152	15.526746	-0.135159	4.293292
703.149837	6313.042277	15.531751	-0.135182	4.290648
702.471741	6305.088831	15.536755	-0.135051	4.288008
702.452004	6297.062451	15.541760	-0.135042	4.285347
702.316499	6289.102411	15.546765	-0.135012	4.282706
702.491961	6281.054596	15.551770	-0.135039	4.280037
702.406809	6273.109750	15.556775	-0.135018	4.277398
702.638814	6265.060015	15.561779	-0.135056	4.274725
702.353463	6257.082525	15.566784	-0.134998	4.272070
702.286495	6249.062039	15.571789	-0.134980	4.269401
702.511033	6241.019969	15.576794	-0.135017	4.266726
702.163377	6233.044357	15.581799	-0.134947	4.264066
701.968338	6225.102455	15.586803	-0.134905	4.261417
702.132241	6217.048984	15.591808	-0.134931	4.258732
702.437388	6209.060193	15.596813	-0.134982	4.256069
702.216973	6201.033070	15.601818	-0.134936	4.253386
702.009890	6193.059299	15.606823	-0.134892	4.250720
702.309774	6185.047286	15.611827	-0.134943	4.248044
702.361570	6177.002529	15.616832	-0.134947	4.245352
701.887761	6169.111303	15.621837	-0.134854	4.242706
702.021434	6161.056666	15.626842	-0.134874	4.240009
701.727347	6153.120143	15.631847	-0.134814	4.237345
702.003214	6145.024051	15.636851	-0.134860	4.234632
702.079350	6137.045882	15.641856	-0.134869	4.231955
702.353230	6129.008308	15.646861	-0.134915	4.229258
702.024223	6121.048613	15.651866	-0.134848	4.226580
701.628123	6113.081281	15.656871	-0.134769	4.223897
701.916302	6105.104901	15.661875	-0.134818	4.221216
702.064307	6097.012633	15.666880	-0.134840	4.218492
701.469717	6089.123436	15.671885	-0.134724	4.215828
701.590978	6081.082177	15.676890	-0.134742	4.213118
702.064103	6073.020294	15.681895	-0.134825	4.210403
701.892728	6065.039085	15.686899	-0.134788	4.207707
701.763860	6057.069121	15.691904	-0.134758	4.205013
702.266061	6049.023371	15.696909	-0.134847	4.202299
702.145890	6041.023704	15.701914	-0.134819	4.199592
701.678057	6033.131703	15.706919	-0.134727	4.196916
701.459340	6025.038761	15.711923	-0.134681	4.194172
701.885770	6016.964321	15.716928	-0.134755	4.191441
701.605895	6008.994454	15.721933	-0.134698	4.188735
701.389683	6001.024086	15.726938	-0.134652	4.186028
701.476748	5993.022284	15.731943	-0.134663	4.183312
701.307378	5985.067249	15.736947	-0.134627	4.180607
701.319347	5977.038855	15.741952	-0.134624	4.177877
701.265493	5969.073883	15.746957	-0.134609	4.175167
701.231110	5961.040116	15.751962	-0.134597	4.172431
700.754357	5953.077091	15.756967	-0.134503	4.169713
700.898490	5945.013054	15.761971	-0.134525	4.166965
700.930005	5936.924312	15.766976	-0.134525	4.164207
701.042134	5929.052079	15.771981	-0.134541	4.161521
700.683890	5921.032238	15.776986	-0.134469	4.158777
700.664236	5913.071727	15.781991	-0.134460	4.156056
700.673386	5905.040606	15.786995	-0.134457	4.153309
700.201780	5897.103868	15.792000	-0.134364	4.150587
700.466301	5889.030590	15.797005	-0.134408	4.147825
700.298054	5881.009047	15.802010	-0.134371	4.145074
700.469819	5873.074403	15.807015	-0.134398	4.142355
700.291765	5865.040245	15.812019	-0.134360	4.139596
700.509843	5857.032555	15.817024	-0.134395	4.136849
700.063177	5849.036256	15.822029	-0.134307	4.134096
700.215957	5841.001645	15.827034	-0.134330	4.131335
700.481962	5833.013515	15.832039	-0.134374	4.128590
700.267241	5825.021270	15.837043	-0.134329	4.125835
700.322542	5817.037957	15.842048	-0.134334	4.123085
700.231901	5809.104361	15.847053	-0.134312	4.120349
699.974052	5801.113641	15.852058	-0.134259	4.117589
700.220593	5793.057725	15.857063	-0.134300	4.114811
700.181398	5785.081291	15.862067	-0.134287	4.112055
699.850033	5777.061845	15.867072	-0.134221	4.109278
699.983986	5769.047176	15.872077	-0.134240	4.106507
699.937759	5761.043945	15.877082	-0.134226	4.103736
699.609623	5753.149916	15.882087	-0.134160	4.100997
699.921411	5745.000383	15.887091	-0.134213	4.098176
699.612674	5737.042681	15.892096	-0.134150	4.095412
699.674399	5729.080350	15.897101	-0.134157	4.092649
699.671149	5721.028917	15.902106	-0.134151	4.089852
699.675450	5713.080570	15.907111	-0.134147	4.087090
699.942233	5704.989796	15.912115	-0.134191	4.084279
699.776873	5697.116471	15.917120	-0.134155	4.081537
699.798561	5689.080548	15.922125	-0.134154	4.078738
699.261301	5681.129284	15.927130	-0.134049	4.075959
699.470664	5673.066365	15.932135	-0.134082	4.073150
699.796181	5665.021149	15.937139	-0.134138	4.070347
699.806790	5657.037231	15.942144	-0.134135	4.067558
699.784201	5649.002122	15.947149	-0.134125	4.064750
699.634423	5641.092995	15.952154	-0.134092	4.061982
699.396696	5633.086890	15.957159	-0.134043	4.059176
699.246424	5625.124634	15.962163	-0.134010	4.056385
698.946995	5617.082503	15.967168	-0.133949	4.053562
699.067776	5609.073666	15.972173	-0.133966	4.050755
698.914004	5601.048245	15.977178	-0.133932	4.047937
699.184709	5593.049414	15.982183	-0.133977	4.045131
698.702596	5585.150563	15.987187	-0.133882	4.042348
698.845011	5577.038701	15.992192	-0.133904	4.039497
698.908695	5569.130134	15.997197	-0.133910	4.036715
698.337306	5561.094286	16.002202	-0.133799	4.033876
698.686795	5552.996571	16.007207	-0.133859	4.031028
698.534571	5545.007917	16.012211	-0.133825	4.028208
698.349054	5537.010481	16.017216	-0.133785	4.025383
698.845564	5529.033552	16.022221	-0.133873	4.022573
698.619095	5521.044761	16.027226	-0.133825	4.019746
698.434893	5513.090686	16.032231	-0.133786	4.016930
698.637389	5504.998793	16.037235	-0.133818	4.014069
698.471698	5497.055221	16.042240	-0.133782	4.011253
698.951688	5489.007897	16.047245	-0.133867	4.008409
698.699422	5481.009113	16.052250	-0.133814	4.005568
698.860396	5473.043824	16.057255	-0.133839	4.002743
698.712524	5465.099158	16.062259	-0.133806	3.999919
698.729668	5457.074415	16.067264	-0.133804	3.997067
698.600144	5449.112205	16.072269	-0.133775	3.994233
698.390352	5441.119107	16.077274	-0.133731	3.991385
698.438367	5433.121524	16.082279	-0.133735	3.988537
698.225775	5425.119973	16.087283	-0.133690	3.985681
698.385631	5417.084842	16.092288	-0.133714	3.982818
698.532786	5409.115481	16.097293	-0.133737	3.979975
698.105425	5401.127489	16.102298	-0.133652	3.977115
698.069928	5393.142465	16.107303	-0.133640	3.974259
697.852526	5385.137886	16.112307	-0.133595	3.971392
697.641173	5377.141511	16.117312	-0.133550	3.968526
697.901865	5369.114291	16.122317	-0.133593	3.965655
697.660647	5361.132770	16.127322	-0.133543	3.962789
697.892211	5353.119345	16.132327	-0.133581	3.959918
697.639213	5345.164860	16.137331	-0.133529	3.957058
697.387414	5337.122374	16.142336	-0.133477	3.954163
697.314887	5329.208126	16.147341	-0.133458	3.951317
697.070978	5321.112075	16.152346	-0.133407	3.948399
697.627680	5313.063859	16.157351	-0.133506	3.945511
697.137170	5305.154017	16.162355	-0.133409	3.942652
697.118868	5297.136509	16.167360	-0.133401	3.939760
697.177469	5289.183306	16.172365	-0.133407	3.936891
697.105450	5281.093832	16.177370	-0.133388	3.933968
697.251059	5273.132377	16.182375	-0.133410	3.931093
697.427056	5265.066425	16.187379	-0.133437	3.928179
697.536018	5257.021017	16.192384	-0.133453	3.925269
697.073395	5249.167597	16.197389	-0.133361	3.922416
696.702655	5241.155237	16.202394	-0.133287	3.919505
696.630503	5233.238555	16.207399	-0.133269	3.916632
696.758498	5225.129952	16.212403	-0.133287	3.913690
696.983196	5217.086798	16.217408	-0.133324	3.910773
696.949563	5209.123118	16.222413	-0.133312	3.907877
696.585787	5201.112307	16.227418	-0.133239	3.904955
696.401469	5193.206221	16.232423	-0.133200	3.902073
696.406768	5185.167593	16.237427	-0.133196	3.899144
695.706794	5177.267335	16.242432	-0.133060	3.896249
695.975604	5169.196077	16.247437	-0.133105	3.893309
696.778405	5161.030556	16.252442	-0.133249	3.890343
696.961641	5153.067172	16.257447	-0.133278	3.887436
696.678896	5145.093743	16.262451	-0.133220	3.884514
696.582751	5137.160718	16.267456	-0.133197	3.881608
696.711613	5129.193395	16.272461	-0.133216	3.878692
696.295679	5121.219024	16.277466	-0.133134	3.875761
696.158836	5113.117425	16.282471	-0.133103	3.872786
696.117468	5105.043247	16.287475	-0.133090	3.869820
695.545180	5097.144561	16.292480	-0.132978	3.866907
695.666671	5089.097601	16.297485	-0.132996	3.863950
696.095842	5081.063495	16.302490	-0.133070	3.861002
696.002250	5073.134675	16.307495	-0.133048	3.858080
695.286491	5065.253307	16.312499	-0.132909	3.855161
695.422258	5057.199520	16.317504	-0.132929	3.852193
695.429810	5049.160764	16.322509	-0.132926	3.849226
695.797983	5041.129050	16.327514	-0.132989	3.846267
696.108324	5033.108318	16.332519	-0.133042	3.843308
696.332995	5025.133070	16.337523	-0.133078	3.840362
696.037025	5017.225461	16.342528	-0.133018	3.837428
695.880724	5009.204056	16.347533	-0.132984	3.834452
695.704255	5001.226293	16.352538	-0.132946	3.831490
695.538182	4993.227277	16.357543	-0.132910	3.828518
695.577285	4985.216012	16.362547	-0.132912	3.825544
695.466665	4977.212063	16.367552	-0.132886	3.822566
695.661596	4969.200883	16.372557	-0.132917	3.819590
695.793092	4961.184470	16.377562	-0.132936	3.816609
695.497650	4953.215945	16.382567	-0.132876	3.813633
695.503150	4945.224430	16.387571	-0.132872	3.810654
695.538056	4937.199807	16.392576	-0.132873	3.807660
695.477298	4929.231417	16.397581	-0.132857	3.804683
695.168448	4921.261427	16.402586	-0.132794	3.801697
695.467162	4913.224237	16.407591	-0.132844	3.798698
695.361335	4905.258208	16.412595	-0.132820	3.795713
695.327541	4897.220888	16.417600	-0.132808	3.792702
695.399907	4889.256859	16.422605	-0.132816	3.789717
695.067362	4881.230272	16.427610	-0.132749	3.786698
694.691913	4873.290944	16.432615	-0.132674	3.783708
694.544112	4865.311071	16.437619	-0.132642	3.780706
694.678440	4857.249127	16.442624	-0.132661	3.777676
694.583727	4849.266407	16.447629	-0.132639	3.774669
694.574302	4841.242639	16.452634	-0.132632	3.771646
694.644605	4833.254364	16.457639	-0.132639	3.768636
694.328797	4825.296187	16.462643	-0.132576	3.765626
694.460630	4817.228485	16.467648	-0.132595	3.762582
694.229090	4809.311123	16.472653	-0.132547	3.759584
693.943730	4801.381247	16.477658	-0.132488	3.756578
693.911688	4793.322543	16.482663	-0.132477	3.753527
694.025043	4785.264626	16.487667	-0.132493	3.750477
694.233437	4777.268994	16.492672	-0.132527	3.747450
694.075004	4769.302790	16.497677	-0.132492	3.744423
693.962122	4761.316403	16.502682	-0.132466	3.741387
693.749747	4753.357624	16.507687	-0.132421	3.738357
693.975800	4745.316881	16.512691	-0.132458	3.735304
693.333061	4737.366586	16.517696	-0.132333	3.732261
693.557980	4729.305443	16.522701	-0.132370	3.729195
693.423428	4721.327860	16.527706	-0.132340	3.726150
693.714390	4713.305011	16.532711	-0.132389	3.723095
693.446223	4705.358133	16.537715	-0.132333	3.720053
693.346138	4697.383348	16.542720	-0.132310	3.717001
693.602869	4689.334947	16.547725	-0.132352	3.713928
693.107299	4681.343620	16.552730	-0.132255	3.710856
693.255700	4673.317975	16.557735	-0.132277	3.707784
693.573424	4665.253680	16.562739	-0.132331	3.704699
693.467437	4657.303421	16.567744	-0.132306	3.701644
693.789759	4649.317801	16.572749	-0.132361	3.698584
693.741029	4641.341213	16.577754	-0.132347	3.695516
693.228507	4633.432773	16.582759	-0.132246	3.692460
693.418094	4625.361375	16.587763	-0.132276	3.689356
693.242097	4617.353399	16.592768	-0.132238	3.686264
693.350963	4609.365571	16.597773	-0.132253	3.683185
692.985016	4601.391104	16.602778	-0.132180	3.680097
692.787893	4593.475963	16.607783	-0.132138	3.677033
693.228195	4585.345483	16.612787	-0.132215	3.673900
692.865862	4577.416207	16.617792	-0.132142	3.670821
692.731693	4569.434002	16.622797	-0.132112	3.667725
692.852078	4561.358424	16.627802	-0.132129	3.664596
692.895454	4553.413946	16.632807	-0.132132	3.661514
692.909900	4545.366442	16.637811	-0.132130	3.658389
692.940416	4537.383315	16.642816	-0.132130	3.655286
692.600791	4529.448420	16.647821	-0.132062	3.652190
692.586781	4521.387397	16.652826	-0.132054	3.649050
692.960912	4513.360159	16.657831	-0.132119	3.645932
692.552281	4505.469845	16.662835	-0.132037	3.642843
692.724036	4497.433397	16.667840	-0.132064	3.639710
692.968239	4489.491391	16.672845	-0.132104	3.636613
692.812055	4481.451553	16.677850	-0.132070	3.633465
692.735013	4473.465038	16.682855	-0.132051	3.630337
692.491461	4465.476432	16.687859	-0.132000	3.627200
692.317367	4457.463695	16.692864	-0.131963	3.624054
692.181711	4449.576948	16.697869	-0.131932	3.620955
692.008481	4441.497087	16.702874	-0.131895	3.617776
692.231102	4433.448689	16.707879	-0.131931	3.614618
692.361528	4425.498656	16.712883	-0.131950	3.611494
692.448145	4417.430208	16.717888	-0.131961	3.608319
691.985252	4409.534053	16.722893	-0.131870	3.605193
692.138857	4401.548494	16.727898	-0.131893	3.602047
692.017258	4393.537496	16.732903	-0.131865	3.598880
691.657647	4385.624225	16.737907	-0.131793	3.595743
691.972888	4377.505879	16.742912	-0.131847	3.592541
692.158475	4369.514395	16.747917	-0.131876	3.589382
692.048860	4361.508031	16.752922	-0.131850	3.586206
692.130929	4353.526304	16.757927	-0.131860	3.583043
691.869923	4345.599487	16.762931	-0.131807	3.579889
691.839322	4337.563131	16.767936	-0.131796	3.576695
691.767868	4329.596616	16.772941	-0.131777	3.573525
691.706495	4321.534541	16.777946	-0.131761	3.570314
691.755446	4313.538961	16.782951	-0.131765	3.567131
691.458217	4305.601990	16.787955	-0.131704	3.563957
691.337966	4297.655166	16.792960	-0.131677	3.560782
691.522650	4289.622459	16.797965	-0.131706	3.557579
691.653816	4281.580613	16.802970	-0.131725	3.554368
691.292211	4273.578210	16.807975	-0.131652	3.551154
691.226630	4265.565665	16.812979	-0.131635	3.547943
691.185557	4257.557008	16.817984	-0.131622	3.544731
691.481270	4249.583873	16.822989	-0.131672	3.541541
691.117223	4241.620325	16.827994	-0.131599	3.538331
690.945202	4233.644172	16.832999	-0.131562	3.535120
690.740676	4225.703417	16.838003	-0.131519	3.531919
691.136182	4217.587051	16.843008	-0.131587	3.528662
691.259114	4209.607222	16.848013	-0.131605	3.525449
690.773800	4201.709855	16.853018	-0.131509	3.522248
690.290136	4193.730131	16.858023	-0.131414	3.519010
690.653761	4185.710461	16.863027	-0.131477	3.515780
690.778784	4177.642383	16.868032	-0.131495	3.512520
690.724549	4169.666517	16.873037	-0.131479	3.509288
690.940254	4161.633192	16.878042	-0.131514	3.506039
691.079299	4153.645490	16.883047	-0.131535	3.502802
690.898771	4145.704642	16.888051	-0.131496	3.499572
690.696266	4137.725333	16.893056	-0.131453	3.496322
690.879511	4129.729436	16.898061	-0.131482	3.493075
690.643507	4121.710240	16.903066	-0.131433	3.489802
690.634437	4113.749705	16.908071	-0.131426	3.486557
690.501886	4105.754332	16.913075	-0.131397	3.483291
690.362608	4097.779284	16.918080	-0.131365	3.480030
690.195734	4089.814735	16.923085	-0.131329	3.476769
690.158141	4081.739913	16.928090	-0.131317	3.473464
690.192721	4073.778291	16.933095	-0.131318	3.470204
690.139249	4065.779413	16.938099	-0.131303	3.466924
689.956408	4057.750590	16.943104	-0.131264	3.463623
690.120722	4049.804193	16.948109	-0.131289	3.460365
690.052227	4041.786035	16.953114	-0.131271	3.457067
690.051304	4033.788312	16.958119	-0.131266	3.453776
689.822558	4025.806047	16.963123	-0.131218	3.450481
689.861495	4017.827213	16.968128	-0.131220	3.447193
689.957005	4009.778029	16.973133	-0.131233	3.443874
689.848297	4001.856706	16.978138	-0.131207	3.440599
689.933804	3993.865981	16.983143	-0.131218	3.437298
689.765115	3985.850933	16.988147	-0.131182	3.433975
689.927310	3977.851215	16.993152	-0.131207	3.430667
690.245332	3969.836538	16.998157	-0.131261	3.427354
689.884803	3961.841072	17.003162	-0.131188	3.424023
689.784776	3953.909387	17.008167	-0.131165	3.420725
689.768380	3945.931201	17.013171	-0.131156	3.417406
689.708642	3937.896160	17.018176	-0.131140	3.414059
689.846374	3929.939463	17.023181	-0.131160	3.410749
689.571641	3921.922351	17.028186	-0.131104	3.407396
689.760785	3913.902868	17.033191	-0.131134	3.404054
689.688122	3905.982567	17.038195	-0.131115	3.400742
689.248035	3898.022570	17.043200	-0.131028	3.397396
689.256025	3890.023197	17.048205	-0.131025	3.394047
689.139554	3881.954380	17.053210	-0.130998	3.390661
688.987857	3873.965088	17.058215	-0.130964	3.387304
689.225281	3865.924043	17.063219	-0.131003	3.383935
689.131601	3857.975454	17.068224	-0.130981	3.380590
689.395249	3849.956881	17.073229	-0.131025	3.377225
689.083067	3841.965718	17.078234	-0.130961	3.373848
688.855580	3834.028004	17.083239	-0.130914	3.370493
688.889669	3826.012288	17.088243	-0.130915	3.367110
688.716904	3818.009105	17.093248	-0.130878	3.363723
688.967446	3810.022600	17.098253	-0.130919	3.360354
689.011901	3802.024198	17.103258	-0.130922	3.356970
688.987414	3794.022141	17.108263	-0.130912	3.353578
689.051922	3786.057991	17.113267	-0.130919	3.350201
688.730806	3778.074379	17.118272	-0.130854	3.346799
688.526134	3770.115322	17.123277	-0.130811	3.343409
688.411479	3762.126514	17.128282	-0.130785	3.340005
688.161879	3754.174568	17.133287	-0.130733	3.336609
688.641587	3746.087829	17.138291	-0.130817	3.333178
688.368607	3738.108992	17.143296	-0.130761	3.329763
688.456408	3730.136631	17.148301	-0.130772	3.326360
688.423840	3722.153108	17.153306	-0.130761	3.322944
688.229411	3714.201612	17.158311	-0.130720	3.319532
687.983376	3706.278983	17.163315	-0.130669	3.316127
687.418305	3698.309330	17.168320	-0.130558	3.312686
687.676191	3690.215346	17.173325	-0.130601	3.309220
688.038577	3682.130552	17.178330	-0.130663	3.305758
687.787653	3674.197386	17.183335	-0.130611	3.302334
687.954805	3666.188730	17.188339	-0.130637	3.298890
687.731269	3658.229981	17.193344	-0.130591	3.295449
687.721180	3650.261156	17.198349	-0.130583	3.292009
687.683237	3642.226654	17.203354	-0.130571	3.288535
687.457032	3634.281880	17.208359	-0.130524	3.285089
687.754220	3626.291633	17.213363	-0.130574	3.281640
687.267774	3618.328285	17.218368	-0.130478	3.278168
686.860893	3610.402317	17.223373	-0.130397	3.274712
687.063699	3602.341684	17.228378	-0.130430	3.271218
687.097000	3594.296454	17.233383	-0.130431	3.267720
687.517890	3586.247969	17.238387	-0.130504	3.264232
687.336914	3578.315397	17.243392	-0.130465	3.260768
687.452871	3570.337573	17.248397	-0.130482	3.257291
687.294937	3562.348457	17.253402	-0.130447	3.253795
687.186776	3554.345571	17.258407	-0.130422	3.250291
687.337618	3546.355906	17.263411	-0.130445	3.246800
687.075148	3538.398155	17.268416	-0.130391	3.243302
686.957153	3530.465564	17.273421	-0.130364	3.239817
686.670906	3522.519585	17.278426	-0.130305	3.236316
686.369810	3514.519860	17.283431	-0.130244	3.232787
685.866151	3506.579167	17.288435	-0.130145	3.229271
686.093484	3498.471912	17.293440	-0.130182	3.225708
686.161288	3490.479036	17.298445	-0.130189	3.222185
686.170201	3482.470737	17.303450	-0.130186	3.218649
686.017767	3474.497046	17.308455	-0.130152	3.215118
685.824731	3466.507124	17.313459	-0.130111	3.211574
686.481315	3458.394938	17.318464	-0.130228	3.208007
686.417299	3450.444265	17.323469	-0.130211	3.204478
686.255540	3442.515196	17.328474	-0.130176	3.200951
685.825659	3434.573472	17.333479	-0.130091	3.197402
686.152425	3426.560812	17.338483	-0.130146	3.193850
685.966373	3418.551348	17.343488	-0.130107	3.190274
685.685650	3410.613906	17.348493	-0.130049	3.186722
686.046297	3402.516920	17.353498	-0.130111	3.183122
686.055661	3394.589076	17.358503	-0.130108	3.179578
685.819936	3386.640024	17.363507	-0.130059	3.176011
685.856427	3378.596405	17.368512	-0.130060	3.172409
685.627182	3370.682254	17.373517	-0.130012	3.168849
684.992174	3362.738665	17.378522	-0.129889	3.165254
685.415363	3354.677227	17.383527	-0.129963	3.161649
685.412666	3346.677365	17.388531	-0.129957	3.158048
685.264906	3338.700794	17.393536	-0.129924	3.154447
685.292033	3330.728058	17.398541	-0.129924	3.150852
685.331905	3322.706507	17.403546	-0.129926	3.147231
685.166550	3314.712257	17.408551	-0.129890	3.143609
685.180401	3306.744825	17.413555	-0.129888	3.140004
684.987946	3298.783474	17.418560	-0.129847	3.136387
685.251191	3290.775381	17.423565	-0.129891	3.132765
685.038593	3282.775437	17.428570	-0.129846	3.129122
684.963556	3274.769905	17.433575	-0.129827	3.125478
685.261830	3266.768860	17.438579	-0.129877	3.121849
684.871222	3258.848987	17.443584	-0.129799	3.118221
684.781082	3250.877104	17.448589	-0.129777	3.114579
684.842415	3242.876916	17.453594	-0.129783	3.110926
684.986095	3234.837604	17.458599	-0.129805	3.107256
685.048201	3226.841115	17.463603	-0.129811	3.103596
684.916464	3218.867393	17.468608	-0.129782	3.099934
684.658865	3210.985170	17.473613	-0.129729	3.096304
684.315681	3202.989257	17.478618	-0.129659	3.092613
684.786334	3194.884831	17.483623	-0.129742	3.088906
684.679062	3186.972390	17.488627	-0.129717	3.085255
684.795904	3178.966122	17.493632	-0.129733	3.081568
684.512041	3171.027699	17.498637	-0.129675	3.077889
684.462931	3163.039903	17.503642	-0.129661	3.074193
684.056143	3155.042313	17.508647	-0.129580	3.070472
684.129835	3147.029043	17.513651	-0.129589	3.066761
684.294408	3138.978470	17.518656	-0.129614	3.063033
684.577832	3130.998612	17.523661	-0.129662	3.059339
684.231426	3123.099747	17.528666	-0.129592	3.055649
684.356253	3115.057528	17.533671	-0.129610	3.051909
683.846417	3107.160225	17.538675	-0.129510	3.048202
683.921320	3099.115399	17.543680	-0.129519	3.044450
683.481154	3091.237963	17.548685	-0.129432	3.040746
683.482253	3083.201203	17.553690	-0.129427	3.036985
683.761444	3075.143471	17.558695	-0.129473	3.033222
683.671100	3067.184650	17.563699	-0.129451	3.029484
683.560259	3059.184045	17.568704	-0.129426	3.025720
683.653109	3051.221232	17.573709	-0.129438	3.021979
683.501355	3043.232917	17.578714	-0.129404	3.018209
683.580108	3035.225827	17.583719	-0.129414	3.014438
683.600542	3027.263931	17.588723	-0.129412	3.010680
683.481830	3019.266570	17.593728	-0.129385	3.006893
683.396512	3011.309439	17.598733	-0.129364	3.003123
683.314880	3003.346814	17.603738	-0.129344	2.999345
683.003253	2995.436392	17.608743	-0.129281	2.995576
683.157729	2987.381532	17.613747	-0.129304	2.991757
683.339326	2979.302513	17.618752	-0.129333	2.987923
683.356706	2971.344935	17.623757	-0.129331	2.984133
683.307125	2963.386943	17.628762	-0.129316	2.980336
683.245268	2955.403194	17.633767	-0.129300	2.976520
682.754017	2947.525312	17.638771	-0.129203	2.972728
682.727283	2939.461908	17.643776	-0.129193	2.968866
682.995256	2931.450214	17.648781	-0.129238	2.965039
682.136954	2923.620746	17.653786	-0.129073	2.961236
682.343139	2915.552542	17.658791	-0.129106	2.957369
682.306464	2907.559935	17.663795	-0.129094	2.953521
682.119872	2899.555158	17.668800	-0.129054	2.949653
682.310965	2891.577545	17.673805	-0.129084	2.945814
682.394066	2883.555460	17.678810	-0.129095	2.941942
682.414152	2875.573324	17.683815	-0.129093	2.938082
682.499486	2867.602281	17.688819	-0.129104	2.934225
682.406496	2859.621282	17.693824	-0.129081	2.930349
682.698810	2851.586234	17.698829	-0.129131	2.926461
682.506885	2843.668053	17.703834	-0.129090	2.922600
682.503385	2835.673112	17.708839	-0.129084	2.918706
682.631038	2827.721754	17.713843	-0.129103	2.914836
682.415831	2819.688986	17.718848	-0.129057	2.910902
682.274004	2811.738847	17.723853	-0.129026	2.907007
682.413199	2803.708452	17.728858	-0.129046	2.903082
682.447631	2795.744360	17.733863	-0.129048	2.899179
682.334902	2787.804133	17.738867	-0.129021	2.895275
682.301647	2779.822051	17.743872	-0.129010	2.891349
682.361867	2771.810628	17.748877	-0.129016	2.887408
682.268057	2763.839324	17.753882	-0.128994	2.883474
682.106343	2755.897287	17.758887	-0.128958	2.879544
682.129131	2747.936680	17.763891	-0.128957	2.875611
681.492693	2740.027500	17.768896	-0.128834	2.871660
681.181484	2732.057754	17.773901	-0.128771	2.867693
681.316640	2723.998678	17.778906	-0.128791	2.863700
681.400340	2716.000506	17.783911	-0.128801	2.859729
681.573068	2708.015249	17.788915	-0.128828	2.855764
681.468295	2700.017308	17.793920	-0.128803	2.851772
681.371599	2692.047209	17.798925	-0.128780	2.847788
681.150705	2684.097423	17.803930	-0.128734	2.843802
680.975531	2676.153704	17.808935	-0.128696	2.839816
680.818904	2668.225345	17.813939	-0.128662	2.835833
680.720379	2660.194057	17.818944	-0.128638	2.831796
680.668575	2652.212378	17.823949	-0.128623	2.827780
680.574313	2644.175655	17.828954	-0.128601	2.823729
680.258399	2636.262581	17.833959	-0.128537	2.819722
680.246061	2628.292679	17.838963	-0.128529	2.815698
680.609155	2620.200256	17.843968	-0.128592	2.811627
680.733988	2612.216447	17.848973	-0.128610	2.807593
681.065190	2604.193755	17.853978	-0.128666	2.803544
680.756774	2596.279187	17.858983	-0.128603	2.799508
680.941270	2588.330137	17.863987	-0.128633	2.795476
680.670751	2580.381542	17.868992	-0.128577	2.791413
680.451175	2572.414280	17.873997	-0.128531	2.787337
680.223850	2564.460306	17.879002	-0.128484	2.783261
680.253479	2556.461301	17.884007	-0.128484	2.779171
680.257403	2548.500807	17.889011	-0.128480	2.775094
679.764502	2540.555419	17.894016	-0.128383	2.770989
680.412789	2532.463410	17.899021	-0.128498	2.766870
680.153483	2524.544827	17.904026	-0.128445	2.762781
680.300016	2516.543764	17.909031	-0.128467	2.758667
679.936929	2508.650254	17.914035	-0.128394	2.754571
679.500220	2500.638540	17.919040	-0.128308	2.750404
679.886629	2492.576281	17.924045	-0.128374	2.746255
679.288323	2484.715984	17.929050	-0.128258	2.742143
679.266013	2476.705770	17.934055	-0.128248	2.737983
679.807635	2468.639559	17.939059	-0.128344	2.733823
679.489586	2460.692985	17.944064	-0.128280	2.729665
679.440268	2452.749404	17.949069	-0.128265	2.725519
678.927052	2444.859569	17.954074	-0.128165	2.721365
678.936510	2436.845044	17.959079	-0.128161	2.717173
679.339238	2428.836274	17.964083	-0.128231	2.713002
678.864458	2420.907978	17.969088	-0.128137	2.708812
678.508406	2412.950653	17.974093	-0.128066	2.704607
678.735878	2404.938654	17.979098	-0.128103	2.700404
678.891638	2396.921013	17.984103	-0.128127	2.696187
678.694427	2388.986199	17.989107	-0.128085	2.691984
678.322297	2381.026641	17.994112	-0.128011	2.687751
679.267292	2372.893828	17.999117	-0.128181	2.683503
678.937777	2365.034360	18.004122	-0.128115	2.679312
678.478578	2357.130921	18.009127	-0.128024	2.675083
678.293329	2349.176432	18.014131	-0.127985	2.670837
678.313457	2341.152317	18.019136	-0.127983	2.666561
678.122325	2333.217091	18.024141	-0.127942	2.662312
678.514778	2325.149795	18.029146	-0.128010	2.658023
678.657496	2317.145669	18.034151	-0.128032	2.653745
678.146427	2309.271181	18.039155	-0.127931	2.649487
678.236082	2301.263000	18.044160	-0.127943	2.645189
678.004404	2293.355127	18.049165	-0.127895	2.640917
678.407851	2285.305538	18.054170	-0.127965	2.636604
678.139873	2277.379477	18.059175	-0.127910	2.632306
678.287770	2269.377908	18.064179	-0.127932	2.627988
678.056303	2261.424855	18.069184	-0.127884	2.623663
678.052893	2253.463951	18.074189	-0.127878	2.619343
677.866956	2245.526512	18.079194	-0.127838	2.615016
678.316533	2237.440767	18.084199	-0.127917	2.610643
678.275037	2229.508119	18.089203	-0.127904	2.606314
677.812054	2221.607575	18.094208	-0.127812	2.601966
678.238770	2213.586519	18.099213	-0.127887	2.597606
678.154101	2205.608250	18.104218	-0.127866	2.593227
678.306680	2197.511503	18.109223	-0.127889	2.588792
678.215216	2189.588483	18.114227	-0.127867	2.584428
678.091645	2181.662267	18.119232	-0.127838	2.580052
678.068148	2173.721702	18.124237	-0.127829	2.575668
677.894010	2165.781504	18.129242	-0.127791	2.571267
678.002680	2157.759851	18.134247	-0.127806	2.566832
678.034011	2149.828408	18.139251	-0.127807	2.562434
677.808163	2141.886449	18.144256	-0.127760	2.558005
677.820669	2133.914400	18.149261	-0.127757	2.553568
677.413601	2126.026583	18.154266	-0.127676	2.549141
677.451585	2117.990800	18.159271	-0.127678	2.544655
677.507324	2110.031834	18.164275	-0.127683	2.540205
677.181905	2102.080076	18.169280	-0.127618	2.535724
677.087233	2094.115559	18.174285	-0.127595	2.531245
676.979509	2086.152449	18.179290	-0.127569	2.526757
677.120739	2078.139513	18.184295	-0.127591	2.522252
677.235384	2070.192283	18.189299	-0.127607	2.517773
677.256619	2062.211021	18.194304	-0.127606	2.513260
676.931248	2054.290383	18.199309	-0.127540	2.508749
677.172554	2046.262983	18.204314	-0.127580	2.504210
676.827020	2038.354616	18.209319	-0.127510	2.499687
676.693493	2030.413346	18.214323	-0.127480	2.495153
676.319507	2022.475126	18.219328	-0.127405	2.490595
676.381598	2014.468054	18.224333	-0.127412	2.486021
676.437142	2006.504838	18.229338	-0.127417	2.481464
676.524640	1998.499329	18.234343	-0.127428	2.476876
676.438559	1990.580320	18.239347	-0.127407	2.472317
676.708281	1982.532848	18.244352	-0.127452	2.467701
676.986715	1974.526678	18.249357	-0.127498	2.463102
676.777328	1966.642327	18.254362	-0.127454	2.458528
676.331889	1958.744236	18.259367	-0.127366	2.453919
676.232576	1950.788382	18.264371	-0.127343	2.449294
676.643933	1942.724373	18.269376	-0.127414	2.444637
676.433657	1934.839276	18.274381	-0.127370	2.440027
676.361540	1926.882841	18.279386	-0.127351	2.435378
676.167251	1918.906579	18.284391	-0.127310	2.430698
675.889914	1910.989787	18.289395	-0.127253	2.426038
675.526926	1903.038095	18.294400	-0.127180	2.421342
675.872227	1895.014154	18.299405	-0.127239	2.416649
676.207952	1886.986729	18.304410	-0.127297	2.411945
676.264070	1879.009314	18.309415	-0.127302	2.407239
675.991486	1871.126853	18.314419	-0.127246	2.402553
675.963389	1863.168370	18.319424	-0.127236	2.397833
675.479856	1855.300889	18.324429	-0.127141	2.393122
675.642114	1847.298294	18.329434	-0.127166	2.388372
675.764669	1839.291460	18.334439	-0.127183	2.383607
675.288156	1831.439436	18.339443	-0.127089	2.378877
675.279855	1823.423693	18.344448	-0.127083	2.374077
675.405467	1815.441995	18.349453	-0.127101	2.369299
675.407852	1807.472170	18.354458	-0.127096	2.364508
675.072929	1799.585779	18.359463	-0.127029	2.359730
675.185029	1791.617144	18.364467	-0.127044	2.354930
675.091359	1783.650771	18.369472	-0.127022	2.350104
675.443574	1775.612559	18.374477	-0.127082	2.345261
674.948916	1767.765025	18.379482	-0.126985	2.340454
675.018243	1759.771137	18.384487	-0.126993	2.335595
675.129751	1751.807004	18.389491	-0.127008	2.330747
675.116833	1743.822994	18.394496	-0.127001	2.325867
674.991967	1735.892418	18.399501	-0.126972	2.321000
675.103695	1727.940092	18.404506	-0.126988	2.316129
674.661151	1720.053446	18.409511	-0.126901	2.311241
674.540875	1712.113507	18.414515	-0.126873	2.306338
674.635953	1704.098079	18.419520	-0.126885	2.301395
674.337834	1696.205772	18.424525	-0.126825	2.296485
673.782907	1688.331718	18.429530	-0.126716	2.291553
674.129292	1680.252581	18.434535	-0.126776	2.286561
674.501289	1672.266144	18.439539	-0.126840	2.281617
674.162141	1664.374631	18.444544	-0.126772	2.276661
674.220969	1656.386336	18.449549	-0.126777	2.271668
674.170192	1648.410861	18.454554	-0.126763	2.266662
674.154573	1640.435239	18.459559	-0.126755	2.261649
674.204021	1632.507117	18.464563	-0.126759	2.256659
673.770279	1624.620554	18.469568	-0.126673	2.251643
673.976897	1616.623600	18.474573	-0.126706	2.246601
673.320338	1608.789586	18.479578	-0.126579	2.241576
673.128127	1600.848285	18.484583	-0.126538	2.236512
673.515148	1592.820712	18.489587	-0.126605	2.231433
673.301476	1584.873149	18.494592	-0.126560	2.226340
673.235272	1576.948783	18.499597	-0.126542	2.221263
673.338784	1568.963753	18.504602	-0.126556	2.216151
673.678475	1560.940756	18.509607	-0.126614	2.211024
673.582527	1553.041343	18.514611	-0.126591	2.205926
673.581522	1545.097105	18.519616	-0.126586	2.200795
673.675565	1537.152637	18.524621	-0.126598	2.195661
673.338661	1529.263660	18.529626	-0.126531	2.190511
673.599183	1521.239948	18.534631	-0.126574	2.185317
673.681322	1513.328357	18.539635	-0.126584	2.180167
673.435421	1505.412117	18.544640	-0.126533	2.174971
673.527916	1497.445832	18.549645	-0.126545	2.169761
673.320090	1489.534761	18.554650	-0.126501	2.164547
673.466654	1481.584715	18.559655	-0.126524	2.159328
672.909600	1473.764505	18.564659	-0.126415	2.154115
672.753132	1465.791005	18.569664	-0.126380	2.148827
672.506104	1457.882426	18.574669	-0.126329	2.143559
672.511214	1449.927471	18.579674	-0.126325	2.138272
672.445794	1441.958786	18.584679	-0.126308	2.132956
672.706249	1433.984338	18.589683	-0.126351	2.127654
672.493198	1426.068920	18.594688	-0.126306	2.122333
672.322392	1418.164611	18.599693	-0.126269	2.117010
672.152536	1410.228730	18.604698	-0.126233	2.111652
671.943625	1402.268150	18.609703	-0.126189	2.106260
672.156891	1394.302877	18.614707	-0.126223	2.100892
672.070399	1386.351615	18.619712	-0.126202	2.095491
672.215876	1378.397748	18.624717	-0.126224	2.090097
671.668154	1370.546133	18.629722	-0.126117	2.084690
671.490907	1362.640798	18.634727	-0.126079	2.079268
671.576359	1354.695815	18.639731	-0.126089	2.073832
671.491959	1346.745561	18.644736	-0.126068	2.068361
670.618813	1338.950502	18.649741	-0.125901	2.062902
670.628274	1330.980018	18.654746	-0.125897	2.057397
670.499549	1323.029039	18.659751	-0.125868	2.051877
670.511553	1315.080444	18.664755	-0.125865	2.046358
670.542403	1307.106839	18.669760	-0.125866	2.040808
670.892717	1299.117674	18.674765	-0.125926	2.035265
670.857434	1291.191442	18.679770	-0.125914	2.029712
670.330959	1283.332087	18.684775	-0.125811	2.024139
670.310257	1275.416485	18.689779	-0.125802	2.018564
670.356058	1267.452848	18.694784	-0.125806	2.012946
670.288429	1259.516296	18.699789	-0.125788	2.007320
670.314308	1251.600664	18.704794	-0.125787	2.001703
670.120230	1243.698716	18.709799	-0.125746	1.996056
670.000194	1235.795146	18.714803	-0.125719	1.990400
669.863183	1227.846325	18.719808	-0.125688	1.984694
669.858788	1219.942347	18.724813	-0.125682	1.979017
669.522889	1212.080651	18.729818	-0.125615	1.973319
669.352723	1204.143323	18.734823	-0.125578	1.967568
669.733264	1196.155911	18.739827	-0.125643	1.961823
669.318141	1188.309096	18.744832	-0.125561	1.956077
668.985374	1180.435643	18.749837	-0.125494	1.950303
669.025849	1172.466531	18.754842	-0.125496	1.944484
669.220589	1164.494811	18.759847	-0.125527	1.938662
668.872442	1156.629482	18.764851	-0.125457	1.932840
668.497544	1148.727259	18.769856	-0.125383	1.926971
668.109991	1140.877646	18.774861	-0.125305	1.921121
668.066897	1132.937543	18.779866	-0.125292	1.915225
667.560322	1125.066534	18.784871	-0.125193	1.909309
667.484635	1117.127009	18.789875	-0.125173	1.903373
667.276973	1109.213799	18.794880	-0.125130	1.897423
666.664940	1101.382874	18.799885	-0.125011	1.891469
666.348892	1093.478283	18.804890	-0.124947	1.885475
666.064606	1085.570933	18.809895	-0.124889	1.879464
665.998940	1077.642585	18.814899	-0.124871	1.873442
665.194805	1069.801373	18.819904	-0.124716	1.867382
665.094677	1061.853688	18.824909	-0.124693	1.861302
664.832052	1053.955281	18.829914	-0.124639	1.855221
664.026649	1046.116930	18.834919	-0.124484	1.849102
663.696031	1038.213500	18.839923	-0.124417	1.842969
662.995283	1030.369775	18.844928	-0.124281	1.836817
662.524624	1022.461888	18.849933	-0.124189	1.830622
662.024237	1014.574333	18.854938	-0.124090	1.824418
661.388609	1006.718144	18.859943	-0.123967	1.818201
660.845225	998.839741	18.864947	-0.123861	1.811957
660.361162	990.914039	18.869952	-0.123765	1.805660
659.275899	983.153320	18.874957	-0.123558	1.799398
658.761051	975.250703	18.879962	-0.123457	1.793071
657.986783	967.334223	18.884967	-0.123308	1.786679
657.732079	959.388414	18.889971	-0.123255	1.780305
656.500194	951.632144	18.894976	-0.123021	1.773937
656.599673	943.586837	18.899981	-0.123034	1.767481
655.508365	935.816492	18.904986	-0.122826	1.761073
654.863116	927.939920	18.909991	-0.122701	1.754612
654.217138	920.076562	18.914995	-0.122575	1.748137
653.168922	912.240239	18.920000	-0.122375	1.741609
652.397142	904.376449	18.925005	-0.122226	1.735068
651.919937	896.467566	18.930010	-0.122132	1.728504
651.042647	888.614109	18.935015	-0.121964	1.721908
650.311038	880.770122	18.940019	-0.121823	1.715314
649.779392	872.861387	18.945024	-0.121718	1.708666
649.228926	864.955343	18.950029	-0.121611	1.701992
648.151169	857.175835	18.955034	-0.121405	1.695328
647.619360	849.253829	18.960039	-0.121301	1.688589
647.001518	841.406128	18.965043	-0.121181	1.681875
646.520650	833.495711	18.970048	-0.121086	1.675099
645.791720	825.649993	18.975053	-0.120945	1.668317
645.714387	817.701763	18.980058	-0.120926	1.661507
644.598059	809.939005	18.985063	-0.120713	1.654687
643.871111	802.095815	18.990067	-0.120572	1.647823
643.438197	794.212285	18.995072	-0.120487	1.640935
642.955473	786.353187	19.000077	-0.120392	1.634033
642.283996	778.484993	19.005082	-0.120262	1.627066
641.761651	770.598496	19.010087	-0.120159	1.620074
641.598668	762.704824	19.015091	-0.120124	1.613097
640.304801	754.977667	19.020096	-0.119878	1.606075
639.688727	747.133758	19.025101	-0.119758	1.599016
639.906848	739.158571	19.030106	-0.119793	1.591927
638.881266	731.397427	19.035111	-0.119597	1.584819
638.177757	723.608966	19.040115	-0.119461	1.577701
637.927766	715.693787	19.045120	-0.119410	1.570502
637.319485	707.868919	19.050125	-0.119291	1.563299
636.690424	700.082545	19.055130	-0.119169	1.556095
635.529397	692.336418	19.060135	-0.118948	1.548815
635.733289	684.354783	19.065139	-0.118981	1.541487
635.185987	676.532647	19.070144	-0.118874	1.534159
634.339416	668.764649	19.075149	-0.118711	1.526801
634.020488	660.919435	19.080154	-0.118647	1.519414
633.352406	653.129148	19.085159	-0.118517	1.511990
632.784754	645.313124	19.090163	-0.118406	1.504520
632.283109	637.500612	19.095168	-0.118308	1.497026
631.986306	629.651283	19.100173	-0.118248	1.489491
631.000930	621.945142	19.105178	-0.118059	1.481947
630.144202	614.189905	19.110183	-0.117895	1.474337
630.042195	606.269948	19.115187	-0.117871	1.466647
629.105699	598.535589	19.120192	-0.117691	1.458964
628.350574	590.763572	19.125197	-0.117545	1.451233
628.151050	582.905736	19.130202	-0.117503	1.443465
627.595061	575.125541	19.135207	-0.117395	1.435674
627.047805	567.350281	19.140211	-0.117288	1.427846
626.524850	559.548418	19.145216	-0.117185	1.419953
626.153575	551.748989	19.150221	-0.117111	1.412043
625.608055	543.986812	19.155226	-0.117005	1.404097
624.369920	536.354558	19.160231	-0.116769	1.396120
624.254392	528.495360	19.165235	-0.116742	1.388056
623.409024	520.772986	19.170240	-0.116580	1.379960
622.776827	513.014410	19.175245	-0.116457	1.371816
622.444936	505.220017	19.180250	-0.116390	1.363638
622.390542	497.379622	19.185255	-0.116375	1.355410
621.550967	489.708779	19.190259	-0.116214	1.347173
620.852795	481.982299	19.195264	-0.116079	1.338850
620.889213	474.139364	19.200269	-0.116081	1.330483
620.555125	466.388837	19.205274	-0.116013	1.322095
620.058573	458.648241	19.210279	-0.115916	1.313634
619.727063	450.834778	19.215283	-0.115849	1.305069
618.511279	443.268872	19.220288	-0.115618	1.296557
618.180409	435.512244	19.225293	-0.115551	1.287941
617.743490	427.799932	19.230298	-0.115465	1.279296
617.312525	420.078129	19.235303	-0.115380	1.270583
616.509492	412.446023	19.240307	-0.115225	1.261840
615.851455	404.779729	19.245312	-0.115098	1.253024
615.523953	397.048887	19.250317	-0.115032	1.244136
614.846516	389.416149	19.255322	-0.114901	1.235229
614.479680	381.695846	19.260327	-0.114827	1.226216
614.183587	373.988073	19.265331	-0.114767	1.217165
613.527530	366.354995	19.270336	-0.114640	1.208061
612.766061	358.748826	19.275341	-0.114493	1.198899
612.563412	351.050239	19.280346	-0.114451	1.189670
612.184301	343.378658	19.285351	-0.114375	1.180364
611.566212	335.781101	19.290355	-0.114255	1.171025
610.824665	328.186644	19.295360	-0.114112	1.161588
610.378147	320.552079	19.300365	-0.114024	1.152087
610.265826	312.854742	19.305370	-0.113998	1.142499
609.148397	305.361705	19.310375	-0.113785	1.132871
608.924328	297.705230	19.315379	-0.113738	1.123146
608.436176	290.124505	19.320384	-0.113643	1.113375
607.813084	282.563899	19.325389	-0.113522	1.103514
607.039634	275.057603	19.330394	-0.113373	1.093600
606.338778	267.514285	19.335399	-0.113237	1.083563
605.364736	260.057869	19.340403	-0.113051	1.073485
604.692165	252.517043	19.345408	-0.112921	1.063267
604.187653	244.969718	19.350413	-0.112822	1.052980
604.135046	237.352135	19.355418	-0.112808	1.042603
603.294962	229.901653	19.360423	-0.112646	1.032163
602.407700	222.471803	19.365427	-0.112476	1.021634
601.982277	214.963182	19.370432	-0.112392	1.010996
601.223152	207.525781	19.375437	-0.112246	1.000264
600.337157	200.123133	19.380442	-0.112076	0.989434
599.583927	192.678062	19.385447	-0.111931	0.978455
598.635011	185.303408	19.390451	-0.111750	0.967404
597.654019	177.946601	19.395456	-0.111562	0.956243
596.019584	170.725433	19.400461	-0.111253	0.944983
594.715949	163.438630	19.405466	-0.111006	0.933573
592.693436	156.270670	19.410471	-0.110625	0.922011
590.658044	149.129502	19.415475	-0.110241	0.910339
586.725922	142.294396	19.420480	-0.109504	0.898472
581.296270	135.663372	19.425485	-0.108489	0.886348
574.035462	129.330797	19.430490	-0.107133	0.874013
564.683167	123.259330	19.435495	-0.105388	0.861320
553.130255	117.489626	19.440499	-0.103233	0.848285
542.244423	111.505334	19.445504	-0.101202	0.834874
533.376656	105.084891	19.450509	-0.099547	0.821099
525.857899	98.423311	19.455514	-0.098142	0.807078
518.521256	91.751433	19.460519	-0.096772	0.792843
512.381522	84.881515	19.465523	-0.095624	0.778369
504.377141	78.582409	19.470528	-0.094130	0.764065