Mon Apr 19 09:35:28 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
4.160398	0.056217	0.000000	0.000101	0.310590

4.362210	0.016541	0.005005	0.000063	0.310576
4.193597	0.051776	0.010010	0.000095	0.310597
4.438598	0.002523	0.015014	0.000049	0.310575
4.045387	0.079091	0.020019	0.000122	0.310599
4.545027	-0.016479	0.025024	0.000029	0.310576
4.600029	-0.027694	0.030029	0.000019	0.310571
4.379784	0.017428	0.035034	0.000060	0.310594
3.959112	0.093393	0.040038	0.000138	0.310592
4.345841	0.023318	0.045043	0.000066	0.310593
4.447667	0.004279	0.050048	0.000048	0.310590
4.536809	-0.013608	0.055053	0.000031	0.310582
4.598717	-0.025603	0.060058	0.000019	0.310579
4.542331	-0.016371	0.065062	0.000030	0.310574
4.667257	-0.037286	0.070067	0.000007	0.310582
4.544020	-0.017077	0.075072	0.000030	0.310572
4.626808	-0.051554	0.080077	0.000014	0.310482
4.720711	-0.123462	0.085082	-0.000003	0.310226
4.527597	-0.088358	0.090086	0.000033	0.310226
4.765253	-0.131187	0.095091	-0.000011	0.310227
4.530839	-0.087325	0.100096	0.000032	0.310233
4.611710	-0.103531	0.105101	0.000017	0.310226
4.527098	-0.085968	0.110106	0.000033	0.310236
4.263835	-0.096633	0.115110	0.000082	0.309963
4.505699	-0.148107	0.120115	0.000037	0.309928
4.330675	-0.118513	0.125120	0.000070	0.309918
4.409493	-0.132255	0.130125	0.000055	0.309920
4.758888	-0.194576	0.135130	-0.000010	0.309926
3.935207	-0.088597	0.140134	0.000143	0.309722
3.964668	-0.117348	0.145139	0.000138	0.309612
4.322698	-0.186238	0.150144	0.000071	0.309594
4.086534	-0.141846	0.155149	0.000115	0.309601
4.725767	-0.261955	0.160154	-0.000004	0.309583
4.368380	-0.257981	0.165158	0.000063	0.309297
4.683363	-0.312931	0.170163	0.000004	0.309308
4.422452	-0.265942	0.175168	0.000053	0.309306
4.645923	-0.333502	0.180173	0.000011	0.309180
4.374663	-0.327484	0.185178	0.000062	0.308977
4.479398	-0.350549	0.190182	0.000042	0.308958
4.448590	-0.341825	0.195187	0.000048	0.308973
4.705097	-0.456358	0.200192	0.000000	0.308655
4.764057	-0.470004	0.205197	-0.000011	0.308641
4.558311	-0.429864	0.210202	0.000028	0.308654
4.520586	-0.492156	0.215206	0.000035	0.308329
4.754806	-0.533904	0.220211	-0.000009	0.308333
4.440835	-0.488204	0.225216	0.000050	0.308280
4.603818	-0.570102	0.230221	0.000019	0.308034
4.530383	-0.553439	0.235226	0.000033	0.308050
4.104724	-0.510297	0.240230	0.000112	0.307889
4.390331	-0.602081	0.245235	0.000059	0.307701
4.085835	-0.542682	0.250240	0.000116	0.307720
3.996424	-0.579759	0.255245	0.000133	0.307470
4.106452	-0.612366	0.260250	0.000112	0.307410
4.415817	-0.690301	0.265254	0.000055	0.307308
4.402637	-0.738482	0.270259	0.000057	0.307070
4.439516	-0.747977	0.275264	0.000050	0.307056
4.129486	-0.744930	0.280269	0.000108	0.306805
4.516202	-0.820661	0.285274	0.000036	0.306779
4.393452	-0.844335	0.290278	0.000059	0.306562
4.321103	-0.855242	0.295283	0.000072	0.306449
4.232102	-0.867055	0.300288	0.000089	0.306316
4.227671	-0.903942	0.305293	0.000090	0.306138
4.148325	-0.908884	0.310298	0.000105	0.306047
3.847083	-0.901561	0.315302	0.000161	0.305822
4.565064	-1.048728	0.320307	0.000027	0.305743
4.737708	-1.122929	0.325312	-0.000005	0.305541
4.309863	-1.070898	0.330317	0.000075	0.305419
5.217956	-1.284582	0.335322	-0.000094	0.305188
5.039531	-1.293956	0.340326	-0.000061	0.304990
4.651689	-1.247242	0.345331	0.000011	0.304877
4.389446	-1.257435	0.350336	0.000060	0.304602
4.544531	-1.300320	0.355341	0.000031	0.304532
5.028333	-1.445981	0.360346	-0.000059	0.304258
4.941136	-1.462527	0.365350	-0.000042	0.304104
5.195444	-1.547373	0.370355	-0.000090	0.303920
4.817057	-1.533162	0.375360	-0.000019	0.303660
4.868542	-1.570776	0.380365	-0.000029	0.303525
4.905741	-1.626450	0.385370	-0.000036	0.303292
4.211526	-1.539487	0.390374	0.000093	0.303105
4.824609	-1.682617	0.395379	-0.000021	0.302953
4.488351	-1.680674	0.400384	0.000042	0.302670
4.561491	-1.733449	0.405389	0.000028	0.302482
5.005184	-1.851381	0.410394	-0.000054	0.302303
4.705278	-1.858923	0.415398	0.000002	0.302006
4.369894	-1.829515	0.420403	0.000064	0.301855
4.951293	-1.975618	0.425408	-0.000044	0.301661
4.941360	-2.031183	0.430413	-0.000042	0.301385
4.771770	-2.048043	0.435418	-0.000010	0.301156
4.602709	-2.058558	0.440422	0.000021	0.300958
4.468668	-2.072997	0.445427	0.000046	0.300771
3.907428	-2.017274	0.450432	0.000151	0.300549
4.050662	-2.087189	0.455437	0.000124	0.300337
3.985749	-2.113871	0.460442	0.000136	0.300152
3.627765	-2.107479	0.465446	0.000203	0.299869
3.158303	-2.066636	0.470451	0.000290	0.299654
3.445675	-2.155431	0.475456	0.000237	0.299477
3.156377	-2.147498	0.480461	0.000291	0.299262
3.343267	-2.237233	0.485466	0.000256	0.298992
2.967479	-2.206098	0.490470	0.000326	0.298812
3.150357	-2.281358	0.495475	0.000292	0.298608
2.467023	-2.215373	0.500480	0.000419	0.298326
2.440543	-2.243922	0.505485	0.000424	0.298164
2.109963	-2.213596	0.510490	0.000486	0.298020
1.456285	-2.168086	0.515494	0.000607	0.297663
0.687061	-2.048086	0.520499	0.000750	0.297567
0.640095	-2.080799	0.525504	0.000759	0.297366
0.248917	-2.055619	0.530509	0.000832	0.297143
0.304460	-2.084859	0.535514	0.000822	0.297050
0.307486	-2.143356	0.540518	0.000821	0.296767
0.466871	-2.194361	0.545523	0.000792	0.296660
-0.127430	-2.129750	0.550528	0.000902	0.296448
-0.053440	-2.185996	0.555533	0.000889	0.296239
-0.267878	-2.164562	0.560538	0.000928	0.296153
-0.350377	-2.217116	0.565542	0.000944	0.295823
-0.220551	-2.256981	0.570547	0.000920	0.295743
-0.259812	-2.288432	0.575552	0.000927	0.295554
-0.945540	-2.214062	0.580557	0.001055	0.295308
-1.624139	-2.106649	0.585562	0.001181	0.295230
-1.510675	-2.187239	0.590566	0.001160	0.294935
-0.829551	-2.331888	0.595571	0.001033	0.294833
-1.274351	-2.302928	0.600576	0.001116	0.294578
-1.431528	-2.305178	0.605581	0.001145	0.294427
-1.191126	-2.370979	0.610586	0.001101	0.294318
-1.136468	-2.444744	0.615590	0.001091	0.294004
-1.360185	-2.431198	0.620595	0.001132	0.293870
-1.284984	-2.489168	0.625600	0.001118	0.293652
-1.168671	-2.556600	0.630605	0.001097	0.293424
-1.486170	-2.526768	0.635610	0.001156	0.293286
-1.960319	-2.493911	0.640614	0.001244	0.293023
-1.910514	-2.539801	0.645619	0.001235	0.292841
-2.124567	-2.530953	0.650624	0.001275	0.292692
-2.394355	-2.539380	0.655629	0.001325	0.292408
-1.606972	-2.709889	0.660634	0.001178	0.292272
-1.757343	-2.729021	0.665638	0.001206	0.292042
-2.370290	-2.668340	0.670643	0.001321	0.291791
-2.569873	-2.658167	0.675648	0.001358	0.291661
-2.195474	-2.776121	0.680653	0.001288	0.291413
-2.301957	-2.801044	0.685658	0.001308	0.291193
-2.369974	-2.823853	0.690662	0.001321	0.291018
-2.188307	-2.904962	0.695667	0.001287	0.290779
-2.571548	-2.875948	0.700672	0.001358	0.290577
-2.969570	-2.835945	0.705677	0.001432	0.290415
-3.080468	-2.858632	0.710682	0.001453	0.290202
-2.873931	-2.949561	0.715686	0.001415	0.289935
-3.968978	-2.777176	0.720691	0.001618	0.289802
-4.343640	-2.758879	0.725696	0.001688	0.289553
-3.989409	-2.859429	0.730701	0.001622	0.289372
-4.166188	-2.846887	0.735706	0.001655	0.289274
-4.832057	-2.793226	0.740710	0.001779	0.288937
-5.323199	-2.721861	0.745715	0.001871	0.288847
-5.766210	-2.682059	0.750720	0.001953	0.288643
-5.652505	-2.737802	0.755725	0.001932	0.288467
-5.963361	-2.713990	0.760730	0.001990	0.288303
-6.474576	-2.660083	0.765734	0.002085	0.288107
-6.902035	-2.598684	0.770739	0.002165	0.288025
-6.254576	-2.769317	0.775744	0.002044	0.287759
-6.386216	-2.764050	0.780749	0.002069	0.287665
-6.487248	-2.802427	0.785754	0.002088	0.287379
-7.077290	-2.706486	0.790758	0.002197	0.287322
-7.431543	-2.699653	0.795763	0.002263	0.287032
-7.762071	-2.644824	0.800768	0.002325	0.287005
-7.636160	-2.722449	0.805773	0.002301	0.286729
-7.713602	-2.719029	0.810778	0.002316	0.286675
-7.932909	-2.736254	0.815782	0.002357	0.286387
-8.322055	-2.675975	0.820787	0.002429	0.286334
-9.114939	-2.579496	0.825792	0.002577	0.286093
-8.972813	-2.609958	0.830797	0.002550	0.286069
-8.583511	-2.741569	0.835802	0.002478	0.285761
-8.780264	-2.709190	0.840806	0.002515	0.285744
-8.866051	-2.741288	0.845811	0.002531	0.285502
-9.040186	-2.709453	0.850816	0.002563	0.285503
-9.358001	-2.716669	0.855821	0.002622	0.285173
-9.871574	-2.619519	0.860826	0.002718	0.285192
-10.166585	-2.627978	0.865830	0.002773	0.284877
-10.325084	-2.602377	0.870835	0.002802	0.284860
-10.195918	-2.670547	0.875840	0.002778	0.284633
-10.906121	-2.564649	0.880845	0.002910	0.284515
-10.910993	-2.582200	0.885850	0.002911	0.284421
-11.704154	-2.468364	0.890854	0.003059	0.284267
-11.347275	-2.535810	0.895859	0.002993	0.284253
-11.739108	-2.527563	0.900864	0.003066	0.283932
-11.627174	-2.550882	0.905869	0.003045	0.283917
-11.359640	-2.634475	0.910874	0.002995	0.283739
-12.361204	-2.478907	0.915878	0.003181	0.283604
-12.621811	-2.430872	0.920883	0.003230	0.283607
-12.694147	-2.479281	0.925888	0.003243	0.283292
-12.895805	-2.443347	0.930893	0.003281	0.283289
-12.538238	-2.531560	0.935898	0.003215	0.283170
-13.140085	-2.455203	0.940902	0.003327	0.283001
-13.043050	-2.473251	0.945907	0.003308	0.282999
-13.141694	-2.512770	0.950912	0.003327	0.282705
-13.983298	-2.366702	0.955917	0.003484	0.282669
-13.818659	-2.403294	0.960922	0.003453	0.282635
-13.844459	-2.455548	0.965926	0.003458	0.282343
-13.637794	-2.493179	0.970931	0.003419	0.282343
-13.952670	-2.466153	0.975936	0.003478	0.282187
-14.334729	-2.432126	0.980941	0.003549	0.282006
-14.154165	-2.462225	0.985946	0.003515	0.282019
-14.279211	-2.488313	0.990950	0.003539	0.281769
-14.608616	-2.438007	0.995955	0.003600	0.281719
-14.099946	-2.548059	1.000960	0.003505	0.281629
-14.443315	-2.535035	1.005965	0.003569	0.281375
-14.687278	-2.487434	1.010970	0.003615	0.281392
-14.870122	-2.499300	1.015974	0.003649	0.281159
-14.953134	-2.498934	1.020979	0.003664	0.281083
-15.422554	-2.417488	1.025984	0.003752	0.281063
-15.652052	-2.432862	1.030989	0.003795	0.280769
-14.875589	-2.576271	1.035994	0.003650	0.280757
-15.237293	-2.534604	1.040998	0.003717	0.280633
-15.681977	-2.475076	1.046003	0.003800	0.280523
-15.783464	-2.454434	1.051008	0.003819	0.280534
-16.066874	-2.465415	1.056013	0.003872	0.280211
-16.572963	-2.373159	1.061018	0.003966	0.280212
-16.366616	-2.430364	1.066022	0.003928	0.280111
-16.556089	-2.442034	1.071027	0.003963	0.279872
-16.708227	-2.413119	1.076032	0.003991	0.279879
-17.383702	-2.315387	1.081037	0.004117	0.279749
-17.086064	-2.408855	1.086042	0.004062	0.279545
-17.405821	-2.349398	1.091046	0.004121	0.279552
-17.594045	-2.341748	1.096051	0.004156	0.279414
-17.661160	-2.356566	1.101056	0.004169	0.279274
-17.685833	-2.354968	1.106061	0.004173	0.279259
-17.627681	-2.403541	1.111066	0.004163	0.279062
-18.803062	-2.213117	1.116070	0.004381	0.278941
-18.456673	-2.275769	1.121075	0.004317	0.278942
-18.158429	-2.366638	1.126080	0.004261	0.278752
-19.286054	-2.184704	1.131085	0.004471	0.278632
-18.808031	-2.271572	1.136090	0.004382	0.278632
-18.853585	-2.288323	1.141094	0.004391	0.278502
-18.957124	-2.308456	1.146099	0.004410	0.278299
-19.391266	-2.227487	1.151104	0.004491	0.278310
-18.990717	-2.322099	1.156109	0.004416	0.278196
-19.378719	-2.283747	1.161114	0.004489	0.278029
-20.213298	-2.131208	1.166118	0.004644	0.278033
-19.619537	-2.255639	1.171123	0.004534	0.277947
-20.007715	-2.234288	1.176128	0.004606	0.277690
-20.197642	-2.202511	1.181133	0.004641	0.277676
-19.957523	-2.247193	1.186138	0.004597	0.277670
-20.402130	-2.224571	1.191142	0.004679	0.277367
-20.802906	-2.148104	1.196147	0.004754	0.277385
-21.359896	-2.043683	1.201152	0.004858	0.277402
-20.997138	-2.155245	1.206157	0.004790	0.277163
-21.248839	-2.127561	1.211162	0.004837	0.277069
-21.324713	-2.117536	1.216166	0.004851	0.277049
-21.280292	-2.137092	1.221171	0.004843	0.276989
-21.244852	-2.186122	1.226176	0.004836	0.276766
-21.470513	-2.146788	1.231181	0.004878	0.276757
-21.268982	-2.186435	1.236186	0.004841	0.276742
-20.948678	-2.309430	1.241190	0.004781	0.276403
-20.598839	-2.375307	1.246195	0.004716	0.276391
-21.182317	-2.287062	1.251200	0.004825	0.276297
-21.594563	-2.249536	1.256205	0.004902	0.276101
-21.024177	-2.353492	1.261210	0.004795	0.276099
-21.861281	-2.233504	1.266214	0.004951	0.275930
-22.223549	-2.193724	1.271219	0.005019	0.275793
-21.976690	-2.236691	1.276224	0.004973	0.275803
-22.130334	-2.239637	1.281229	0.005001	0.275641
-22.264499	-2.233581	1.286234	0.005026	0.275545
-21.985245	-2.286222	1.291238	0.004974	0.275535
-22.173222	-2.302197	1.296243	0.005009	0.275271
-22.701020	-2.218540	1.301248	0.005108	0.275206
-22.492365	-2.259460	1.306253	0.005069	0.275190
-22.446359	-2.323992	1.311258	0.005060	0.274895
-22.788406	-2.266113	1.316262	0.005124	0.274872
-23.130170	-2.213930	1.321267	0.005188	0.274819
-23.117812	-2.262535	1.326272	0.005185	0.274575
-23.141022	-2.263425	1.331277	0.005190	0.274548
-23.308250	-2.255319	1.336282	0.005221	0.274430
-23.452963	-2.263056	1.341286	0.005248	0.274250
-23.103721	-2.326791	1.346291	0.005183	0.274249
-23.472721	-2.302053	1.351296	0.005252	0.274025
-23.579147	-2.303695	1.356301	0.005271	0.273914
-23.173772	-2.381378	1.361306	0.005196	0.273893
-24.375780	-2.214494	1.366310	0.005420	0.273620
-24.232008	-2.241714	1.371315	0.005393	0.273614
-24.089151	-2.284371	1.376320	0.005366	0.273526
-24.479608	-2.257455	1.381325	0.005439	0.273292
-24.656500	-2.222266	1.386330	0.005472	0.273308
-24.774959	-2.227237	1.391334	0.005494	0.273167
-25.168844	-2.182811	1.396339	0.005567	0.273023
-25.492507	-2.122731	1.401344	0.005628	0.273029
-25.606625	-2.131244	1.406349	0.005649	0.272874
-25.106944	-2.258753	1.411354	0.005556	0.272680
-25.196955	-2.244180	1.416358	0.005573	0.272670
-25.221269	-2.281359	1.421363	0.005577	0.272449
-25.134818	-2.316418	1.426368	0.005561	0.272346
-25.018014	-2.346382	1.431373	0.005540	0.272300
-25.536652	-2.302842	1.436378	0.005636	0.272029
-25.702932	-2.273661	1.441382	0.005667	0.272024
-25.906228	-2.259930	1.446387	0.005705	0.271900
-26.592256	-2.161678	1.451392	0.005833	0.271759
-26.737499	-2.134113	1.456397	0.005860	0.271765
-26.193576	-2.269089	1.461402	0.005758	0.271572
-26.650818	-2.216401	1.466406	0.005844	0.271410
-26.809335	-2.187748	1.471411	0.005873	0.271409
-26.564660	-2.274677	1.476416	0.005828	0.271182
-26.832981	-2.240231	1.481421	0.005878	0.271105
-26.885526	-2.233649	1.486426	0.005887	0.271090
-27.084121	-2.255253	1.491430	0.005924	0.270781
-26.743139	-2.318550	1.496435	0.005861	0.270774
-27.083726	-2.277012	1.501440	0.005924	0.270665
-27.866649	-2.159919	1.506445	0.006070	0.270529
-27.491309	-2.226803	1.511450	0.006000	0.270537
-27.884709	-2.197286	1.516454	0.006073	0.270312
-28.251117	-2.151485	1.521459	0.006142	0.270200
-27.810858	-2.233048	1.526464	0.006060	0.270192
-28.023274	-2.246631	1.531469	0.006099	0.269912
-28.570383	-2.150860	1.536474	0.006201	0.269892
-28.356341	-2.196420	1.541478	0.006161	0.269856
-27.985284	-2.323372	1.546483	0.006092	0.269537
-28.111702	-2.299816	1.551488	0.006116	0.269540
-28.891646	-2.184204	1.556493	0.006261	0.269399
-28.867217	-2.212403	1.561498	0.006257	0.269271
-28.244537	-2.330229	1.566502	0.006141	0.269246
-29.355153	-2.178264	1.571507	0.006347	0.268977
-29.670845	-2.127409	1.576512	0.006406	0.268941
-29.525205	-2.154983	1.581517	0.006379	0.268935
-29.311045	-2.251319	1.586522	0.006339	0.268626
-29.784454	-2.167820	1.591526	0.006427	0.268612
-29.646183	-2.208387	1.596531	0.006402	0.268529
-29.941704	-2.196313	1.601536	0.006457	0.268304
-30.257043	-2.139959	1.606541	0.006515	0.268299
-30.711786	-2.071476	1.611546	0.006600	0.268222
-30.798251	-2.091162	1.616550	0.006616	0.268030
-30.689242	-2.113507	1.621555	0.006596	0.268017
-30.643136	-2.144887	1.626560	0.006587	0.267892
-30.861216	-2.145603	1.631565	0.006628	0.267674
-30.749735	-2.164817	1.636570	0.006607	0.267680
-30.976749	-2.159893	1.641574	0.006650	0.267483
-30.715318	-2.234593	1.646579	0.006601	0.267336
-30.976519	-2.183283	1.651584	0.006650	0.267356
-31.548940	-2.134892	1.656589	0.006756	0.267054
-31.479121	-2.152273	1.661594	0.006743	0.267029
-31.283038	-2.194240	1.666598	0.006707	0.266994
-32.058750	-2.095824	1.671603	0.006851	0.266763
-32.017095	-2.103465	1.676608	0.006843	0.266762
-32.364169	-2.052096	1.681613	0.006908	0.266698
-32.335434	-2.107383	1.686618	0.006903	0.266426
-31.995975	-2.173382	1.691622	0.006839	0.266403
-31.388900	-2.312250	1.696627	0.006727	0.266248
-31.768618	-2.271793	1.701632	0.006797	0.266093
-32.598892	-2.119877	1.706637	0.006952	0.266097
-32.234512	-2.239954	1.711642	0.006884	0.265804
-32.099690	-2.272010	1.716646	0.006859	0.265763
-32.791175	-2.161906	1.721651	0.006988	0.265678
-32.844716	-2.181636	1.726656	0.006998	0.265517
-32.570891	-2.234460	1.731661	0.006947	0.265500
-32.494975	-2.294687	1.736666	0.006933	0.265247
-33.346392	-2.153645	1.741670	0.007091	0.265172
-32.904802	-2.246892	1.746675	0.007009	0.265101
-32.897898	-2.294189	1.751680	0.007008	0.264849
-33.350914	-2.213702	1.756685	0.007092	0.264839
-33.273692	-2.267190	1.761690	0.007078	0.264623
-33.256595	-2.290909	1.766694	0.007074	0.264510
-33.451984	-2.270046	1.771699	0.007111	0.264429
-33.734614	-2.254967	1.776704	0.007164	0.264230
-33.458639	-2.308052	1.781709	0.007112	0.264214
-33.647035	-2.322443	1.786714	0.007147	0.263948
-34.097489	-2.251879	1.791718	0.007231	0.263885
-34.060307	-2.280345	1.796723	0.007224	0.263766
-34.135501	-2.298003	1.801728	0.007238	0.263594
-34.571207	-2.219488	1.806733	0.007319	0.263590
-34.569104	-2.274222	1.811738	0.007319	0.263291
-34.975634	-2.204259	1.816742	0.007395	0.263269
-35.131786	-2.194377	1.821747	0.007424	0.263167
-34.972252	-2.258096	1.826752	0.007394	0.262976
-35.145445	-2.227717	1.831757	0.007426	0.262969
-35.089138	-2.286382	1.836762	0.007416	0.262702
-35.575152	-2.209229	1.841766	0.007506	0.262640
-35.775530	-2.187250	1.846771	0.007544	0.262560
-35.809502	-2.221559	1.851776	0.007550	0.262337
-36.024318	-2.183658	1.856781	0.007590	0.262330
-35.964742	-2.233194	1.861786	0.007579	0.262117
-36.083392	-2.232311	1.866790	0.007601	0.262002
-36.110422	-2.234450	1.871795	0.007606	0.261963
-36.456159	-2.215123	1.876800	0.007671	0.261722
-36.255089	-2.255931	1.881805	0.007633	0.261698
-36.804260	-2.184887	1.886810	0.007735	0.261539
-37.709520	-2.045958	1.891814	0.007904	0.261396
-37.061929	-2.166195	1.896819	0.007783	0.261382
-37.056305	-2.207186	1.901824	0.007782	0.261161
-37.792303	-2.087322	1.906829	0.007919	0.261083
-37.380799	-2.166340	1.911834	0.007843	0.261060
-37.416561	-2.215234	1.916838	0.007849	0.260752
-37.047236	-2.283177	1.921843	0.007781	0.260748
-37.615234	-2.201517	1.926848	0.007886	0.260627
-38.406528	-2.074832	1.931853	0.008034	0.260531
-38.357260	-2.079642	1.936858	0.008025	0.260554
-38.762894	-2.055936	1.941862	0.008100	0.260276
-38.901261	-2.044059	1.946867	0.008126	0.260202
-38.473839	-2.122844	1.951872	0.008046	0.260196
-38.329561	-2.208630	1.956877	0.008020	0.259864
-38.748458	-2.130823	1.961882	0.008098	0.259873
-39.003268	-2.100804	1.966886	0.008145	0.259782
-39.215476	-2.104417	1.971891	0.008185	0.259546
-39.382260	-2.073417	1.976896	0.008216	0.259550
-39.899983	-2.001140	1.981901	0.008312	0.259427
-39.261009	-2.146553	1.986906	0.008193	0.259265
-39.231249	-2.154126	1.991910	0.008188	0.259252
-39.333877	-2.185755	1.996915	0.008207	0.258971
-39.349636	-2.199804	2.001920	0.008210	0.258876

-39.950685	-2.137811	2.011917	0.008322	0.258611
-39.925601	-2.175939	2.021914	0.008317	0.258423
-40.071088	-2.175483	2.031910	0.008344	0.258277
-40.372589	-2.163621	2.041907	0.008400	0.258036
-40.160009	-2.210673	2.051904	0.008361	0.257989
-40.461122	-2.204618	2.061901	0.008417	0.257715
-40.847408	-2.145199	2.071898	0.008489	0.257653
-40.705179	-2.172207	2.081894	0.008462	0.257647
-40.746149	-2.217422	2.091891	0.008470	0.257351
-41.163492	-2.143253	2.101888	0.008548	0.257340
-41.303099	-2.117621	2.111885	0.008574	0.257342
-41.265912	-2.123133	2.121882	0.008567	0.257349
-41.751152	-2.033323	2.131878	0.008657	0.257357
-41.625013	-2.055616	2.141875	0.008634	0.257360
-41.126501	-2.148794	2.151872	0.008541	0.257346
-41.761376	-2.030463	2.161869	0.008659	0.257362
-41.372680	-2.101967	2.171866	0.008587	0.257358
-41.998180	-1.986696	2.181862	0.008703	0.257366
-41.927396	-1.997917	2.191859	0.008690	0.257375
-41.739517	-2.034470	2.201856	0.008655	0.257361
-41.245715	-2.093328	2.211853	0.008563	0.257535
-40.992333	-2.117341	2.221850	0.008516	0.257659
-41.317655	-2.055960	2.231846	0.008577	0.257672
-40.839580	-2.146528	2.241843	0.008488	0.257651
-40.938579	-2.125006	2.251840	0.008506	0.257671
-40.793167	-2.092867	2.261837	0.008479	0.258000
-40.970268	-2.057166	2.271834	0.008512	0.258019
-41.627863	-1.928531	2.281830	0.008634	0.258070
-41.433675	-1.918127	2.291827	0.008598	0.258326
-41.251273	-1.952565	2.301824	0.008564	0.258319
-40.934643	-1.952716	2.311821	0.008505	0.258641
-40.363021	-2.059466	2.321818	0.008399	0.258625
-40.075005	-2.074495	2.331814	0.008346	0.258834
-39.925742	-2.085736	2.341811	0.008318	0.258923
-40.296732	-1.989555	2.351808	0.008387	0.259083
-40.137283	-1.982485	2.361805	0.008357	0.259285
-40.167213	-1.946013	2.371802	0.008363	0.259458
-40.195236	-1.920352	2.381798	0.008368	0.259572
-39.805525	-1.943131	2.391795	0.008295	0.259841
-39.609063	-1.963983	2.401792	0.008259	0.259923
-39.334854	-1.961314	2.411789	0.008208	0.260216
-39.266547	-1.947059	2.421786	0.008195	0.260364
-38.782146	-2.001198	2.431782	0.008105	0.260553
-38.910411	-1.948622	2.441779	0.008129	0.260715
-38.925997	-1.923969	2.451776	0.008132	0.260836
-37.819831	-2.078615	2.461773	0.007926	0.261095
-38.149288	-1.993942	2.471770	0.007987	0.261232
-38.287191	-1.932430	2.481766	0.008013	0.261433
-37.965696	-1.938224	2.491763	0.007953	0.261725
-37.470142	-2.006845	2.501760	0.007861	0.261844
-37.266887	-2.008663	2.511757	0.007823	0.262038
-37.072906	-1.999314	2.521754	0.007787	0.262285
-37.152467	-1.957107	2.531750	0.007802	0.262438
-36.837060	-1.969570	2.541747	0.007743	0.262685
-36.689714	-1.948491	2.551744	0.007716	0.262949
-36.133422	-2.022260	2.561741	0.007612	0.263100
-36.417630	-1.931590	2.571738	0.007665	0.263314
-35.947325	-1.968277	2.581734	0.007578	0.263582
-35.998409	-1.923117	2.591731	0.007587	0.263779
-35.848062	-1.912292	2.601728	0.007559	0.263989
-35.526791	-1.915941	2.611725	0.007499	0.264289
-34.899034	-1.994107	2.621722	0.007383	0.264486
-34.803799	-1.982134	2.631718	0.007365	0.264646
-34.232134	-2.044904	2.641715	0.007258	0.264872
-34.179861	-2.006237	2.651712	0.007249	0.265135
-33.575941	-2.086670	2.661709	0.007136	0.265295
-33.695751	-2.021187	2.671706	0.007159	0.265533
-33.408432	-2.033780	2.681702	0.007105	0.265749
-32.785126	-2.121921	2.691699	0.006989	0.265887
-32.952629	-2.051902	2.701696	0.007020	0.266102
-32.982358	-1.992447	2.711693	0.007026	0.266396
-32.158894	-2.112958	2.721690	0.006873	0.266555
-31.592469	-2.185121	2.731686	0.006767	0.266722
-31.662293	-2.123829	2.741683	0.006780	0.266986
-31.099429	-2.203518	2.751680	0.006676	0.267109
-30.903308	-2.198284	2.761677	0.006639	0.267330
-30.907844	-2.154698	2.771674	0.006640	0.267561
-30.482465	-2.207043	2.781670	0.006561	0.267697
-30.585358	-2.133318	2.791667	0.006580	0.267994
-30.447892	-2.122395	2.801664	0.006554	0.268188
-29.869407	-2.198350	2.811661	0.006447	0.268346
-29.793310	-2.165070	2.821658	0.006433	0.268600
-29.686590	-2.140287	2.831654	0.006413	0.268838
-30.255269	-1.997439	2.841651	0.006519	0.269050
-29.422926	-2.108513	2.851648	0.006364	0.269266
-28.993265	-2.136461	2.861645	0.006284	0.269536
-29.001019	-2.093520	2.871642	0.006285	0.269759
-28.729020	-2.105938	2.881638	0.006235	0.269958
-28.874517	-2.034915	2.891635	0.006262	0.270196
-28.641929	-2.012442	2.901632	0.006218	0.270543
-28.280793	-2.043927	2.911629	0.006151	0.270726
-27.975578	-2.063491	2.921626	0.006094	0.270918
-28.144610	-1.985812	2.931622	0.006126	0.271169
-27.964157	-1.968919	2.941619	0.006092	0.271434
-27.512769	-1.993318	2.951616	0.006008	0.271741
-27.408286	-1.970056	2.961613	0.005989	0.271966
-27.314762	-1.939439	2.971610	0.005971	0.272219
-26.757744	-1.995745	2.981606	0.005868	0.272458
-26.759839	-1.947019	2.991603	0.005868	0.272715
-26.493072	-1.933653	3.001600	0.005818	0.273043
-26.110626	-1.958404	3.011597	0.005747	0.273281
-25.367741	-2.054356	3.021594	0.005609	0.273488
-25.296361	-2.024248	3.031590	0.005596	0.273716
-24.654598	-2.101868	3.041587	0.005476	0.273922
-24.361564	-2.096609	3.051584	0.005422	0.274231
-24.527514	-2.027871	3.061581	0.005453	0.274435
-24.016508	-2.081962	3.071578	0.005358	0.274639
-23.917773	-2.052581	3.081574	0.005339	0.274889
-24.088066	-1.964741	3.091571	0.005371	0.275188
-23.521915	-2.020252	3.101568	0.005266	0.275437
-23.709445	-1.943090	3.111565	0.005300	0.275663
-23.588336	-1.922322	3.121562	0.005278	0.275888
-23.538951	-1.877214	3.131558	0.005269	0.276171
-23.726603	-1.787751	3.141555	0.005304	0.276461
-23.229406	-1.816114	3.151552	0.005211	0.276786
-22.860454	-1.834018	3.161549	0.005142	0.277043
-22.080201	-1.928245	3.171546	0.004997	0.277292
-21.779803	-1.935933	3.181542	0.004941	0.277536
-21.662764	-1.910224	3.191539	0.004920	0.277781
-21.244690	-1.936360	3.201536	0.004842	0.278041
-20.577870	-2.006462	3.211533	0.004718	0.278307
-19.968723	-2.079636	3.221530	0.004604	0.278502
-20.084713	-2.018780	3.231526	0.004626	0.278709
-19.945934	-1.998921	3.241523	0.004600	0.278943
-19.636743	-1.993019	3.251520	0.004543	0.279265
-19.117713	-2.051894	3.261517	0.004446	0.279449
-18.859876	-2.063301	3.271514	0.004398	0.279632
-18.614777	-2.060810	3.281510	0.004352	0.279876
-18.345571	-2.058381	3.291507	0.004302	0.280141
-18.258493	-2.031339	3.301504	0.004286	0.280362
-17.657517	-2.106539	3.311501	0.004174	0.280538
-17.089895	-2.166532	3.321498	0.004069	0.280761
-17.096416	-2.132840	3.331494	0.004070	0.280928
-16.933737	-2.126951	3.341491	0.004040	0.281111
-16.912496	-2.075347	3.351488	0.004036	0.281396
-16.960066	-2.018482	3.361485	0.004044	0.281644
-16.908175	-1.985118	3.371482	0.004035	0.281864
-16.574572	-2.004531	3.381478	0.003973	0.282075
-16.334898	-1.992112	3.391475	0.003928	0.282362
-16.080297	-1.983976	3.401472	0.003881	0.282641
-15.492518	-2.048906	3.411469	0.003771	0.282856
-15.487139	-2.005456	3.421466	0.003770	0.283083
-15.360637	-1.985349	3.431462	0.003747	0.283303
-15.287770	-1.936129	3.441459	0.003733	0.283622
-14.901988	-1.960153	3.451456	0.003661	0.283857
-14.483896	-1.991739	3.461453	0.003584	0.284083
-14.490862	-1.941599	3.471450	0.003585	0.284332
-14.363100	-1.918011	3.481446	0.003561	0.284570
-14.086412	-1.905785	3.491443	0.003510	0.284888
-13.640021	-1.939542	3.501440	0.003427	0.285129
-12.819840	-2.047852	3.511437	0.003274	0.285335
-12.649881	-2.034448	3.521434	0.003242	0.285560
-12.431633	-2.027431	3.531430	0.003202	0.285796
-12.509614	-1.968415	3.541427	0.003216	0.286023
-11.875603	-2.044160	3.551424	0.003098	0.286223
-11.545280	-2.065107	3.561421	0.003037	0.286421
-11.357826	-2.034945	3.571418	0.003002	0.286745
-11.026723	-2.056758	3.581414	0.002940	0.286938
-11.026870	-2.021213	3.591411	0.002940	0.287117
-11.016569	-1.968258	3.601408	0.002938	0.287393
-10.745411	-1.961362	3.611405	0.002888	0.287676
-10.767622	-1.910991	3.621402	0.002892	0.287909
-9.871578	-2.033432	3.631398	0.002725	0.288112
-9.488399	-2.064317	3.641395	0.002654	0.288307
-9.408203	-2.020006	3.651392	0.002639	0.288602
-9.290591	-2.001509	3.661389	0.002617	0.288802
-8.923229	-2.025245	3.671386	0.002549	0.289017
-9.066573	-1.945467	3.681382	0.002576	0.289286
-8.828003	-1.937313	3.691379	0.002531	0.289544
-8.882164	-1.878763	3.701376	0.002541	0.289787
-8.244023	-1.945584	3.711373	0.002423	0.290032
-7.525913	-2.037148	3.721370	0.002289	0.290226
-7.421958	-1.989776	3.731366	0.002270	0.290557
-7.338177	-1.970740	3.741363	0.002254	0.290727
-7.395018	-1.920151	3.751360	0.002265	0.290927
-7.156974	-1.914287	3.761357	0.002220	0.291171
-6.952921	-1.896061	3.771354	0.002182	0.291446
-6.960410	-1.833453	3.781350	0.002184	0.291750
-6.844735	-1.809671	3.791347	0.002162	0.291972
-6.748246	-1.771795	3.801344	0.002144	0.292246
-6.378048	-1.787873	3.811341	0.002075	0.292500
-6.223125	-1.757145	3.821338	0.002046	0.292791
-5.208715	-1.889144	3.831334	0.001858	0.293049
-5.073683	-1.862106	3.841331	0.001833	0.293304
-4.828913	-1.864853	3.851328	0.001787	0.293510
-5.021392	-1.776882	3.861325	0.001823	0.293771
-5.387969	-1.648811	3.871322	0.001891	0.294073
-4.919959	-1.677967	3.881318	0.001804	0.294348
-4.677988	-1.670650	3.891315	0.001759	0.294600
-4.477875	-1.642598	3.901312	0.001722	0.294916
-3.914234	-1.684592	3.911309	0.001617	0.295212
-3.608040	-1.683442	3.921306	0.001560	0.295491
-3.687216	-1.621002	3.931302	0.001574	0.295726
-3.800694	-1.547482	3.941299	0.001596	0.295984
-3.746183	-1.497865	3.951296	0.001585	0.296275
-3.598074	-1.457698	3.961293	0.001558	0.296602
-3.861937	-1.339733	3.971290	0.001607	0.296944
-2.789078	-1.476075	3.981286	0.001407	0.297229
-2.854901	-1.400708	3.991283	0.001420	0.297537
-2.724101	-1.359870	4.001280	0.001395	0.297851
-2.908961	-1.255623	4.011277	0.001430	0.298194
-2.827800	-1.204999	4.021274	0.001414	0.298511
-2.637937	-1.170354	4.031270	0.001379	0.298846
-2.528197	-1.115672	4.041267	0.001359	0.299207
-2.187536	-1.112932	4.051264	0.001295	0.299519
-1.796046	-1.110815	4.061261	0.001222	0.299873
-1.984902	-1.001261	4.071258	0.001257	0.300236
-2.208959	-0.876197	4.081254	0.001299	0.300642
-1.671620	-0.912569	4.091251	0.001199	0.300937
-1.627723	-0.846300	4.101248	0.001191	0.301293
-1.520536	-0.784536	4.111245	0.001171	0.301683
-1.619005	-0.695180	4.121242	0.001189	0.302025
-1.262143	-0.668973	4.131238	0.001123	0.302461
-1.181276	-0.602597	4.141235	0.001108	0.302849
-0.723717	-0.608901	4.151232	0.001023	0.303215
-0.799430	-0.509396	4.161229	0.001037	0.303624
-1.178928	-0.342902	4.171226	0.001107	0.304089
-0.620727	-0.362675	4.181222	0.001003	0.304477
-0.690591	-0.266454	4.191219	0.001016	0.304873
-0.383286	-0.227578	4.201216	0.000959	0.305322
-0.319051	-0.156090	4.211213	0.000947	0.305716
-0.147002	-0.099179	4.221210	0.000915	0.306133
0.000000	-0.029959	4.231206	0.000888	0.306586

0.004476	0.242241	4.236211	0.000887	0.307872
0.340573	0.736084	4.241216	0.000824	0.310469
1.050280	1.452187	4.246221	0.000691	0.314382
2.362531	2.345465	4.251226	0.000446	0.319548
2.634395	3.723362	4.256230	0.000395	0.325946
3.243677	5.337662	4.261235	0.000280	0.333515
3.827158	7.252160	4.266240	0.000170	0.342168
4.873316	9.396315	4.271245	-0.000026	0.351898
6.032919	11.825027	4.276250	-0.000243	0.362586
7.024875	14.621817	4.281254	-0.000430	0.374275
8.822435	17.598519	4.286259	-0.000766	0.386829
9.811408	21.067773	4.291264	-0.000953	0.400241
12.031620	24.671088	4.296269	-0.001368	0.414464
14.607227	28.567614	4.301274	-0.001851	0.429420
16.075215	33.025373	4.306278	-0.002127	0.445046
17.469142	37.864655	4.311283	-0.002389	0.461295
18.704255	43.087299	4.316288	-0.002623	0.478064
19.572677	48.730799	4.321293	-0.002788	0.495301
20.451534	54.723858	4.326298	-0.002956	0.512949
21.577395	60.990212	4.331302	-0.003169	0.530875
22.949548	67.552028	4.336307	-0.003429	0.549110
22.823300	74.701392	4.341312	-0.003410	0.567568
24.075871	81.895354	4.346317	-0.003648	0.586167
24.996090	89.428327	4.351322	-0.003825	0.604860
25.592821	97.298989	4.356326	-0.003941	0.623641
26.146935	105.431346	4.361331	-0.004049	0.642444
28.312029	113.495035	4.366336	-0.004458	0.661191
32.238567	121.493410	4.371341	-0.005194	0.679951
33.650102	130.160228	4.376346	-0.005462	0.698657
35.258830	138.960734	4.381350	-0.005768	0.717215
36.587272	147.984849	4.386355	-0.006021	0.735645
37.800681	157.157425	4.391360	-0.006253	0.753868
39.619615	166.349973	4.396365	-0.006597	0.771899
41.120771	175.695280	4.401370	-0.006883	0.789693
42.533886	185.147770	4.406374	-0.007152	0.807258
43.889464	194.691719	4.411379	-0.007411	0.824590
44.816908	204.350207	4.416384	-0.007590	0.841631
45.461112	214.071277	4.421389	-0.007716	0.858354
46.489897	223.742860	4.426394	-0.007914	0.874787
47.675500	233.387887	4.431398	-0.008141	0.890917
48.953572	243.036155	4.436403	-0.008385	0.906791
49.083352	252.860185	4.441408	-0.008416	0.922351
50.144180	262.484275	4.446413	-0.008620	0.937596
51.977346	271.957384	4.451418	-0.008967	0.952571
52.386926	281.651651	4.456422	-0.009050	0.967273
53.239850	291.240537	4.461427	-0.009215	0.981713
54.248147	300.758984	4.466432	-0.009409	0.995880
54.910495	310.264428	4.471437	-0.009538	1.009742
56.078492	319.645608	4.476442	-0.009762	1.023366
57.295410	328.972381	4.481446	-0.009994	1.036745
58.549141	338.265740	4.486451	-0.010234	1.049916
59.410728	347.548084	4.491456	-0.010400	1.062816
60.205201	356.825066	4.496461	-0.010554	1.075537
62.492305	365.767084	4.501466	-0.010986	1.088007
63.225902	374.979719	4.506470	-0.011129	1.100338
64.354113	384.077691	4.511475	-0.011345	1.112471
64.951979	393.201715	4.516480	-0.011462	1.124389
66.246713	402.166972	4.521485	-0.011709	1.136132
66.796832	411.240690	4.526490	-0.011817	1.147729
68.014345	420.122218	4.531494	-0.012049	1.159113
68.698667	429.084734	4.536499	-0.012183	1.170374
69.350696	437.975505	4.541504	-0.012310	1.181432
70.436566	446.763281	4.546509	-0.012518	1.192352
71.975426	455.439349	4.551514	-0.012810	1.203131
72.483844	464.286321	4.556518	-0.012910	1.213808
74.595692	472.822903	4.561523	-0.013309	1.224347
75.999266	481.460930	4.566528	-0.013576	1.234773
77.313432	490.096867	4.571533	-0.013826	1.245091
78.407605	498.772028	4.576538	-0.014036	1.255326
79.574284	507.379153	4.581542	-0.014259	1.265414
80.539883	516.014705	4.586547	-0.014444	1.275415
80.915951	524.699843	4.591552	-0.014520	1.285282
81.769068	533.305128	4.596557	-0.014684	1.295074
83.656321	541.698561	4.601562	-0.015041	1.304751
84.862362	550.268381	4.606566	-0.015271	1.314423
85.419525	558.867797	4.611571	-0.015381	1.323937
86.137019	567.404093	4.616576	-0.015520	1.333344
86.674989	575.936896	4.621581	-0.015625	1.342649
87.673286	584.373401	4.626586	-0.015817	1.351869
88.256029	592.853566	4.631590	-0.015931	1.360999
89.549100	601.210550	4.636595	-0.016177	1.370062
90.882732	609.554404	4.641600	-0.016431	1.379059
92.577999	617.840526	4.646605	-0.016752	1.388000
94.043200	626.191669	4.651610	-0.017030	1.396910
94.609093	634.650880	4.656614	-0.017141	1.405721
96.291262	642.940342	4.661619	-0.017459	1.414492
97.515019	651.298924	4.666624	-0.017693	1.423202
98.548443	659.688320	4.671629	-0.017891	1.431857
99.590335	668.042199	4.676634	-0.018090	1.440426
100.129675	676.479051	4.681638	-0.018196	1.448944
101.218149	684.817448	4.686643	-0.018404	1.457403
102.491082	693.085962	4.691648	-0.018646	1.465775
103.813721	701.404331	4.696653	-0.018898	1.474156
106.058626	709.522879	4.701658	-0.019321	1.482441
107.513310	717.783681	4.706662	-0.019598	1.490692
107.576078	726.317579	4.711667	-0.019615	1.498940
108.669732	734.609433	4.716672	-0.019824	1.507072
110.235503	742.819825	4.721677	-0.020121	1.515157
110.604582	751.222593	4.726682	-0.020195	1.523195
111.643318	759.493950	4.731686	-0.020394	1.531170
113.030938	767.731239	4.736691	-0.020658	1.539124
113.929777	776.039332	4.741696	-0.020830	1.547029
115.331465	784.235814	4.746701	-0.021097	1.554866
115.658336	792.609264	4.751706	-0.021163	1.562665
116.616089	800.829087	4.756710	-0.021347	1.570378
118.060749	809.027354	4.761715	-0.021621	1.578105
119.034346	817.278993	4.766720	-0.021808	1.585774
119.534479	825.626270	4.771725	-0.021906	1.593422
121.182122	833.739033	4.776730	-0.022218	1.600989
122.575600	841.908169	4.781734	-0.022483	1.608534
124.023383	850.100926	4.786739	-0.022758	1.616072
124.994552	858.387845	4.791744	-0.022944	1.623590
125.952196	866.661452	4.796749	-0.023128	1.631060
127.857762	874.751301	4.801754	-0.023488	1.638466
129.188451	882.895633	4.806758	-0.023741	1.645806
129.877674	891.227168	4.811763	-0.023875	1.653187
130.656283	899.469465	4.816768	-0.024025	1.660470
132.560901	907.572252	4.821773	-0.024385	1.667755
134.564293	915.654127	4.826778	-0.024763	1.675003
135.433731	923.919148	4.831782	-0.024930	1.682222
136.419871	932.172715	4.836787	-0.025119	1.689416
137.494578	940.391430	4.841792	-0.025325	1.696561
138.378906	948.631305	4.846797	-0.025495	1.703668
139.621278	956.824996	4.851802	-0.025732	1.710754
141.056296	964.944768	4.856806	-0.026004	1.717774
142.239083	973.137762	4.861811	-0.026230	1.724793
143.295699	981.337842	4.866816	-0.026432	1.731773
144.395315	989.535642	4.871821	-0.026642	1.738727
145.444919	997.729749	4.876826	-0.026843	1.745644
146.787264	1005.904552	4.881830	-0.027098	1.752556
147.997529	1014.064954	4.886835	-0.027328	1.759411
149.206976	1022.211914	4.891840	-0.027559	1.766228
149.928764	1030.472204	4.896845	-0.027699	1.773048
151.030019	1038.628387	4.901850	-0.027909	1.779806
152.201036	1046.782039	4.906854	-0.028132	1.786544
153.199968	1055.022034	4.911859	-0.028324	1.793305
154.264374	1063.133679	4.916864	-0.028527	1.799945
155.489904	1071.259176	4.921869	-0.028761	1.806592
156.823494	1079.401829	4.926874	-0.029014	1.813241
157.356164	1087.633455	4.931878	-0.029119	1.819837
158.132489	1095.847345	4.936883	-0.029269	1.826425
159.326173	1103.961917	4.941888	-0.029496	1.832962
159.998131	1112.140053	4.946893	-0.029627	1.839462
161.194807	1120.271782	4.951898	-0.029855	1.845965
162.599120	1128.361892	4.956902	-0.030122	1.852438
163.752766	1136.519750	4.961907	-0.030342	1.858911
164.799940	1144.629525	4.966912	-0.030542	1.865311
166.303732	1152.722135	4.971917	-0.030827	1.871729
167.661879	1160.828593	4.976922	-0.031085	1.878119
168.787244	1168.941320	4.981926	-0.031300	1.884464
169.706051	1177.135890	4.986931	-0.031477	1.890825
170.598092	1185.305250	4.991936	-0.031648	1.897143
171.480260	1193.458816	4.996941	-0.031817	1.903427
173.045473	1201.544207	5.001946	-0.032114	1.909716
173.919507	1209.720044	5.006950	-0.032282	1.915973
175.496103	1217.775691	5.011955	-0.032581	1.922200
175.659396	1226.069280	5.016960	-0.032617	1.928424
176.028132	1234.281840	5.021965	-0.032691	1.934590
176.879660	1242.420519	5.026970	-0.032855	1.940737
177.310539	1250.599194	5.031974	-0.032940	1.946846
177.758288	1258.789570	5.036979	-0.033029	1.952946
178.788567	1266.812224	5.041984	-0.033226	1.958968
180.395634	1274.807291	5.046989	-0.033530	1.965015
181.395481	1282.939546	5.051994	-0.033722	1.971077
182.179422	1291.073275	5.056998	-0.033873	1.977097
183.296801	1299.158546	5.062003	-0.034086	1.983100
184.209358	1307.297300	5.067008	-0.034262	1.989100
185.005120	1315.429554	5.072013	-0.034415	1.995066
186.408503	1323.467045	5.077018	-0.034682	2.001010
187.193403	1331.599902	5.082022	-0.034833	2.006938
187.992010	1339.772690	5.087027	-0.034987	2.012879
188.868809	1347.895693	5.092032	-0.035156	2.018775
189.569709	1356.023390	5.097037	-0.035291	2.024638
190.392909	1364.138224	5.102042	-0.035450	2.030488
191.126758	1372.234737	5.107046	-0.035592	2.036299
191.939442	1380.344916	5.112051	-0.035748	2.042110
191.434746	1388.667485	5.117056	-0.035660	2.047918
192.485905	1396.701704	5.122061	-0.035861	2.053668
193.441249	1404.775403	5.127066	-0.036044	2.059419
194.458840	1412.781831	5.132070	-0.036239	2.065113
194.834151	1420.987064	5.137075	-0.036314	2.070865
195.230049	1429.148702	5.142080	-0.036393	2.076572
196.681316	1437.098257	5.147085	-0.036668	2.082223
197.755815	1445.170633	5.152090	-0.036874	2.087905
198.737229	1453.247211	5.157094	-0.037062	2.093565
199.298736	1461.410082	5.162099	-0.037171	2.099227
200.081196	1469.502850	5.167104	-0.037322	2.104848
200.437601	1477.705373	5.172109	-0.037394	2.110486
201.089571	1485.845744	5.177114	-0.037521	2.116096
202.237428	1493.812444	5.182118	-0.037740	2.121621
203.578234	1501.817208	5.187123	-0.037995	2.127177
204.070701	1509.985645	5.192128	-0.038092	2.132745
204.614615	1518.126442	5.197133	-0.038198	2.138286
205.748821	1526.145905	5.202138	-0.038415	2.143787
206.260558	1534.295475	5.207142	-0.038515	2.149301
207.037944	1542.385708	5.212147	-0.038665	2.154787
207.895470	1550.453815	5.217152	-0.038830	2.160252
209.131818	1558.441328	5.222157	-0.039065	2.165685
209.458051	1566.667829	5.227162	-0.039132	2.171176
209.211546	1574.898766	5.232166	-0.039091	2.176602
209.847174	1582.973873	5.237171	-0.039215	2.181995
210.647234	1591.045560	5.242176	-0.039369	2.187388
212.050452	1599.017999	5.247181	-0.039635	2.192758
213.309229	1607.042048	5.252186	-0.039875	2.198136
213.939855	1615.127733	5.257190	-0.039998	2.203481
214.212918	1623.339278	5.262195	-0.040054	2.208863
215.650325	1631.304344	5.267200	-0.040327	2.214178
216.203648	1639.428671	5.272205	-0.040435	2.219503
218.126952	1647.345962	5.277210	-0.040798	2.224806
218.747114	1655.509644	5.282214	-0.040919	2.230136
219.423089	1663.640376	5.287219	-0.041050	2.235437
220.110967	1671.735038	5.292224	-0.041183	2.240703
221.080330	1679.774217	5.297229	-0.041369	2.245947
221.577338	1687.947640	5.302234	-0.041467	2.251222
222.421826	1696.009525	5.307238	-0.041629	2.256444
223.239985	1704.093894	5.312243	-0.041787	2.261665
224.085840	1712.158027	5.317248	-0.041950	2.266864
224.692951	1720.289075	5.322253	-0.042068	2.272073
225.872940	1728.315857	5.327258	-0.042293	2.277253
226.642347	1736.358095	5.332262	-0.042442	2.282396
227.020901	1744.508705	5.337267	-0.042517	2.287560
227.504701	1752.623645	5.342272	-0.042613	2.292700
228.707572	1760.613377	5.347277	-0.042842	2.297812
229.300385	1768.731704	5.352282	-0.042957	2.302940
230.404891	1776.718638	5.357286	-0.043168	2.308019
231.477216	1784.772055	5.362291	-0.043373	2.313124
231.832664	1792.941294	5.367296	-0.043445	2.318229
232.701438	1800.946918	5.372301	-0.043612	2.323265
234.049500	1808.970546	5.377306	-0.043868	2.328342
234.803132	1817.073463	5.382310	-0.044014	2.333406
235.905443	1825.122769	5.387315	-0.044224	2.338455
236.617718	1833.230236	5.392320	-0.044362	2.343496
237.722411	1841.280030	5.397325	-0.044573	2.348523
238.152163	1849.470060	5.402330	-0.044658	2.353569
238.424309	1857.584187	5.407334	-0.044714	2.358545
239.546309	1865.554454	5.412339	-0.044928	2.363493
240.374489	1873.623638	5.417344	-0.045088	2.368466
240.832067	1881.737809	5.422349	-0.045178	2.373425
241.303910	1889.855988	5.427354	-0.045271	2.378377
241.981792	1897.894563	5.432358	-0.045403	2.383288
242.705883	1905.979480	5.437363	-0.045543	2.388220
243.090395	1914.115837	5.442368	-0.045620	2.393145
244.354782	1922.041510	5.447373	-0.045860	2.398005
244.849968	1930.166787	5.452378	-0.045958	2.402912
245.489007	1938.225461	5.457382	-0.046082	2.407781
246.722664	1946.225601	5.462387	-0.046317	2.412652
247.385641	1954.323629	5.467392	-0.046446	2.417526
247.698249	1962.427023	5.472397	-0.046509	2.422366
248.813659	1970.468742	5.477402	-0.046722	2.427222
249.598339	1978.541160	5.482406	-0.046873	2.432061
250.066437	1986.666098	5.487411	-0.046966	2.436896
250.765135	1994.715708	5.492416	-0.047101	2.441696
251.799610	2002.699759	5.497421	-0.047299	2.446473
252.821106	2010.754515	5.502426	-0.047494	2.451281
253.566864	2018.824260	5.507430	-0.047638	2.456067
253.881274	2026.966773	5.512435	-0.047702	2.460852
254.699400	2035.003976	5.517440	-0.047860	2.465606
255.927760	2043.005793	5.522445	-0.048094	2.470361
257.364673	2050.995963	5.527450	-0.048367	2.475116
258.002989	2059.096456	5.532454	-0.048491	2.479864
259.222374	2067.094876	5.537459	-0.048723	2.484588
259.927637	2075.214786	5.542464	-0.048859	2.489335
260.209827	2083.378692	5.547469	-0.048917	2.494065
261.603754	2091.337151	5.552474	-0.049182	2.498752
262.026919	2099.455755	5.557478	-0.049266	2.503449
262.626229	2107.570041	5.562483	-0.049383	2.508148
263.074855	2115.689429	5.567488	-0.049472	2.512830
263.224488	2123.813970	5.572493	-0.049505	2.517484
264.672970	2131.702434	5.577498	-0.049780	2.522090
265.554533	2139.714440	5.582502	-0.049949	2.526716
265.983529	2147.873349	5.587507	-0.050034	2.531384
266.317354	2155.970306	5.592512	-0.050102	2.536001
266.946761	2164.033831	5.597517	-0.050224	2.540613
267.786104	2172.064784	5.602522	-0.050386	2.545212
268.673259	2180.095822	5.607526	-0.050556	2.549806
269.504959	2188.147328	5.612531	-0.050716	2.554400
270.094109	2196.215597	5.617536	-0.050831	2.558977
271.084308	2204.169937	5.622541	-0.051021	2.563511
272.107026	2212.204870	5.627546	-0.051216	2.568084
272.357257	2220.345262	5.632550	-0.051268	2.572652
272.754133	2228.481987	5.637555	-0.051347	2.577221
273.229240	2236.535722	5.642560	-0.051441	2.581741
274.275116	2244.510983	5.647565	-0.051641	2.586249
274.813114	2252.687585	5.652570	-0.051746	2.590826
275.887358	2260.694450	5.657574	-0.051952	2.595337
276.238361	2268.771253	5.662579	-0.052022	2.599829
276.531282	2276.833038	5.667584	-0.052082	2.604301
276.696264	2284.913565	5.672589	-0.052118	2.608766
276.835088	2293.049933	5.677594	-0.052149	2.613253
277.499380	2301.019259	5.682598	-0.052278	2.617677
278.189363	2309.028899	5.687603	-0.052412	2.622116
278.325275	2317.136385	5.692608	-0.052442	2.626564
278.695184	2325.200879	5.697613	-0.052516	2.630997
279.042939	2333.284819	5.702618	-0.052586	2.635431
279.205471	2341.324379	5.707622	-0.052622	2.639821
279.505401	2349.337440	5.712627	-0.052683	2.644198
280.274842	2357.362358	5.717632	-0.052831	2.648606
280.346192	2365.457545	5.722637	-0.052850	2.652999
280.843936	2373.510792	5.727642	-0.052948	2.657389
280.835180	2381.595986	5.732646	-0.052952	2.661756
281.373014	2389.609970	5.737651	-0.053057	2.666113
281.841449	2397.668534	5.742656	-0.053149	2.670483
282.401367	2405.682883	5.747661	-0.053259	2.674827
282.868522	2413.725429	5.752666	-0.053351	2.679174
283.458602	2421.685259	5.757670	-0.053466	2.683477
283.563864	2429.807227	5.762675	-0.053491	2.687828
284.488079	2437.811250	5.767680	-0.053668	2.692162
284.522383	2445.936760	5.772685	-0.053680	2.696496
285.089848	2453.987859	5.777690	-0.053791	2.700819
285.607149	2461.992418	5.782694	-0.053892	2.705106
286.416198	2470.003594	5.787699	-0.054048	2.709408
286.600521	2478.112185	5.792704	-0.054088	2.713715
286.966131	2486.162319	5.797709	-0.054161	2.717996
287.554956	2494.188473	5.802714	-0.054276	2.722272
287.542462	2502.301547	5.807718	-0.054279	2.726548
288.294330	2510.294812	5.812723	-0.054424	2.730803
288.983106	2518.319831	5.817728	-0.054558	2.735064
289.669484	2526.303874	5.822733	-0.054691	2.739297
289.814536	2534.479718	5.827738	-0.054723	2.743589
290.324681	2542.500163	5.832742	-0.054823	2.747816
290.914675	2550.566844	5.837747	-0.054938	2.752066
291.115079	2558.654219	5.842752	-0.054981	2.756296
290.964830	2566.745868	5.847757	-0.054958	2.760499
291.988170	2574.647889	5.852762	-0.055154	2.764670
292.122023	2582.730043	5.857766	-0.055184	2.768874
292.009822	2590.871648	5.862771	-0.055168	2.773087
292.940058	2598.802095	5.867776	-0.055347	2.777247
293.123890	2606.871348	5.872781	-0.055386	2.781428
293.806122	2614.879872	5.877786	-0.055518	2.785601
294.187009	2622.936688	5.882790	-0.055595	2.789775
294.746087	2630.981322	5.887795	-0.055704	2.793946
294.775467	2639.098895	5.892800	-0.055715	2.798117
295.100827	2647.107010	5.897805	-0.055780	2.802244
296.005514	2655.084153	5.902810	-0.055954	2.806383
295.722447	2663.240812	5.907814	-0.055907	2.810536
296.338975	2671.241484	5.912819	-0.056027	2.814658
296.801729	2679.261610	5.917824	-0.056118	2.818774
297.268239	2687.256469	5.922829	-0.056210	2.822871
297.281228	2695.408932	5.927834	-0.056218	2.827016
297.190116	2703.505954	5.932838	-0.056206	2.831120
297.783678	2711.526139	5.937843	-0.056322	2.835220
298.613522	2719.426837	5.942848	-0.056481	2.839267
298.930099	2727.459260	5.947853	-0.056546	2.843344
299.406824	2735.529663	5.952858	-0.056640	2.847444
299.457721	2743.652513	5.957862	-0.056654	2.851540
299.920441	2751.674964	5.962867	-0.056746	2.855604
300.795872	2759.619881	5.967872	-0.056914	2.859646
301.132933	2767.683115	5.972877	-0.056982	2.863711
301.829143	2775.702326	5.977882	-0.057117	2.867768
302.054224	2783.775355	5.982886	-0.057164	2.871820
302.550529	2791.813023	5.987891	-0.057262	2.875863
303.108546	2799.846560	5.992896	-0.057371	2.879903
303.395345	2807.890862	5.997901	-0.057429	2.883926
303.383880	2816.046646	6.002906	-0.057432	2.887983
304.444558	2823.962205	6.007910	-0.057635	2.891974
304.226719	2832.113052	6.012915	-0.057600	2.896006
304.388831	2840.182856	6.017920	-0.057635	2.900013
304.819471	2848.171436	6.022925	-0.057721	2.903989
305.184069	2856.248755	6.027930	-0.057794	2.907999
305.213201	2864.362700	6.032934	-0.057805	2.912004
305.227571	2872.472354	6.037939	-0.057812	2.916000
305.406632	2880.459969	6.042944	-0.057851	2.919939
305.730548	2888.394129	6.047949	-0.057916	2.923855
305.988388	2896.456552	6.052954	-0.057970	2.927825
306.356825	2904.492373	6.057958	-0.058044	2.931783
307.027047	2912.474136	6.062963	-0.058174	2.935725
307.685717	2920.447805	6.067968	-0.058301	2.939656
308.225515	2928.454506	6.072973	-0.058407	2.943593
308.563824	2936.557734	6.077978	-0.058475	2.947560
308.891957	2944.626964	6.082982	-0.058542	2.951504
309.038707	2952.699311	6.087987	-0.058574	2.955436
309.621834	2960.691875	6.092992	-0.058688	2.959346
309.879626	2968.722941	6.097997	-0.058741	2.963253
310.493411	2976.713883	6.103002	-0.058861	2.967153
310.790584	2984.818445	6.108006	-0.058921	2.971087
311.275738	2992.838546	6.113011	-0.059017	2.974984
311.374029	3000.923466	6.118016	-0.059040	2.978888
311.476174	3008.962842	6.123021	-0.059065	2.982764
312.409234	3016.947481	6.128026	-0.059244	2.986653
313.050993	3024.962568	6.133030	-0.059368	2.990535
313.293748	3033.038305	6.138035	-0.059419	2.994421
313.444815	3041.142295	6.143040	-0.059452	2.998311
313.612444	3049.140198	6.148045	-0.059489	3.002146
313.932269	3057.194987	6.153050	-0.059553	3.006010
314.159644	3065.219077	6.158054	-0.059601	3.009851
314.725997	3073.235936	6.163059	-0.059712	3.013700
314.443636	3081.378167	6.168064	-0.059664	3.017561
314.964944	3089.330723	6.173069	-0.059767	3.021367
315.263069	3097.395444	6.178074	-0.059827	3.025211
315.970211	3105.360305	6.183078	-0.059964	3.029022
316.290495	3113.426379	6.188083	-0.060029	3.032858
317.021802	3121.410835	6.193088	-0.060170	3.036670
317.458706	3129.428607	6.198093	-0.060257	3.040478
317.850821	3137.458700	6.203098	-0.060335	3.044286
318.396277	3145.502954	6.208102	-0.060442	3.048102
318.606088	3153.619754	6.213107	-0.060486	3.051932
319.002571	3161.651682	6.218112	-0.060565	3.055726
319.202373	3169.664290	6.223117	-0.060608	3.059496
319.574515	3177.727026	6.228122	-0.060682	3.063294
319.588001	3185.812346	6.233126	-0.060690	3.067080
319.840386	3193.876348	6.238131	-0.060742	3.070863
319.859669	3201.989815	6.243136	-0.060751	3.074653
320.316645	3209.901574	6.248141	-0.060841	3.078365
320.802691	3217.883844	6.253146	-0.060937	3.082107
320.921958	3225.963970	6.258150	-0.060964	3.085873
321.719518	3233.889282	6.263155	-0.061118	3.089594
322.470961	3241.899261	6.268160	-0.061263	3.093347
323.027994	3249.914219	6.273165	-0.061372	3.097089
323.350154	3258.050730	6.278170	-0.061437	3.100872
323.933342	3266.003366	6.283174	-0.061551	3.104577
323.857229	3274.148845	6.288179	-0.061542	3.108336
324.295704	3282.174314	6.293184	-0.061629	3.112059
324.585358	3290.211745	6.298189	-0.061688	3.115776
325.073037	3298.221361	6.303194	-0.061784	3.119485
325.277752	3306.244712	6.308198	-0.061828	3.123183
325.458583	3314.295725	6.313203	-0.061867	3.126888
325.787854	3322.353801	6.318208	-0.061933	3.130598
326.135244	3330.370019	6.323213	-0.062003	3.134286
326.280033	3338.486374	6.328218	-0.062035	3.138006
326.726711	3346.451172	6.333222	-0.062124	3.141666
327.247513	3354.458516	6.338227	-0.062226	3.145344
327.662925	3362.486627	6.343232	-0.062308	3.149023
328.157955	3370.506871	6.348237	-0.062406	3.152697
328.310934	3378.603436	6.353242	-0.062440	3.156386
328.431656	3386.619904	6.358246	-0.062467	3.160033
329.154165	3394.572806	6.363251	-0.062607	3.163674
329.404195	3402.651183	6.368256	-0.062659	3.167347
329.684802	3410.713305	6.373261	-0.062716	3.171009
330.350688	3418.728618	6.378266	-0.062845	3.174662
330.565361	3426.766360	6.383270	-0.062891	3.178302
331.060101	3434.794498	6.388275	-0.062988	3.181945
331.741303	3442.790424	6.393280	-0.063120	3.185578
332.418067	3450.781681	6.398285	-0.063251	3.189204
332.725229	3458.884124	6.403290	-0.063314	3.192860
333.373863	3466.858722	6.408294	-0.063440	3.196469
333.886574	3474.894753	6.413299	-0.063540	3.200096
334.183625	3482.944152	6.418304	-0.063601	3.203715
334.768705	3490.962625	6.423309	-0.063715	3.207328
335.134748	3499.068706	6.428314	-0.063788	3.210967
335.579212	3507.089930	6.433318	-0.063876	3.214568
335.703025	3515.136224	6.438323	-0.063905	3.218161
335.972435	3523.193861	6.443328	-0.063960	3.221762
336.388937	3531.180005	6.448333	-0.064043	3.225333
336.655807	3539.282153	6.453338	-0.064098	3.228946
336.449379	3547.339045	6.458342	-0.064065	3.232514
337.480719	3555.253484	6.463347	-0.064262	3.236068
337.534796	3563.298739	6.468352	-0.064277	3.239634
338.462245	3571.194617	6.473357	-0.064455	3.243166
338.735891	3579.321980	6.478362	-0.064511	3.246770
338.737221	3587.399796	6.483366	-0.064517	3.250337
338.871822	3595.447846	6.488371	-0.064547	3.253892
339.316211	3603.497897	6.493376	-0.064635	3.257456
339.399096	3611.545874	6.498381	-0.064656	3.261001
339.896879	3619.520827	6.503386	-0.064753	3.264527
340.723093	3627.477812	6.508390	-0.064912	3.268055
341.121392	3635.567365	6.513395	-0.064992	3.271619
341.120154	3643.682803	6.518400	-0.064997	3.275175
341.752401	3651.586080	6.523405	-0.065120	3.278659
342.385729	3659.607297	6.528410	-0.065243	3.282192
342.501436	3667.709192	6.533414	-0.065270	3.285735
342.984409	3675.686090	6.538419	-0.065365	3.289234
343.817715	3683.697844	6.543424	-0.065525	3.292758
344.309756	3691.756105	6.548429	-0.065622	3.296285
344.399337	3699.859784	6.553434	-0.065644	3.299813
344.976674	3707.837388	6.558438	-0.065757	3.303300
345.631021	3715.826108	6.563443	-0.065884	3.306792
346.278638	3723.866727	6.568448	-0.066010	3.310303
346.631982	3731.895794	6.573453	-0.066081	3.313793
346.986741	3739.955044	6.578458	-0.066152	3.317292
346.953980	3748.064939	6.583462	-0.066151	3.320795
347.945456	3755.923898	6.588467	-0.066341	3.324225
348.145693	3764.036657	6.593472	-0.066383	3.327730
348.088089	3772.148390	6.598477	-0.066378	3.331222
348.663668	3780.141946	6.603482	-0.066490	3.334683
348.835073	3788.183545	6.608486	-0.066527	3.338145
349.292567	3796.194462	6.613491	-0.066618	3.341602
349.936066	3804.176367	6.618496	-0.066743	3.345050
350.065239	3812.225958	6.623501	-0.066772	3.348503
350.278506	3820.321062	6.628506	-0.066817	3.351976
351.109042	3828.255865	6.633510	-0.066977	3.355400
351.120356	3836.325671	6.638515	-0.066984	3.358847
351.590889	3844.368835	6.643520	-0.067077	3.362296
352.165007	3852.345515	6.648525	-0.067189	3.365717
352.612845	3860.353301	6.653530	-0.067278	3.369143
352.415188	3868.479011	6.658534	-0.067246	3.372592
352.703466	3876.512857	6.663539	-0.067305	3.376016
353.414305	3884.514133	6.668544	-0.067443	3.379438
353.847635	3892.490298	6.673549	-0.067528	3.382836
354.096682	3900.579746	6.678554	-0.067580	3.386272
354.201800	3908.638199	6.683558	-0.067605	3.389686
354.360519	3916.703946	6.688563	-0.067640	3.393101
354.988010	3924.686145	6.693568	-0.067762	3.396495
355.677345	3932.618804	6.698573	-0.067895	3.399867
356.397250	3940.634894	6.703578	-0.068034	3.403271
356.653705	3948.718648	6.708582	-0.068087	3.406683
356.925958	3956.749891	6.713587	-0.068143	3.410071
357.158987	3964.812636	6.718592	-0.068192	3.413467
358.065735	3972.732355	6.723597	-0.068366	3.416824
357.792150	3980.882252	6.728602	-0.068320	3.420232
358.518897	3988.829652	6.733606	-0.068461	3.423587
358.974499	3996.864567	6.738611	-0.068551	3.426965
359.373628	4004.934008	6.743616	-0.068630	3.430353
359.778772	4012.909416	6.748621	-0.068711	3.433698
359.986430	4021.004995	6.753626	-0.068755	3.437083
360.122026	4029.008221	6.758630	-0.068785	3.440424
360.412398	4037.012521	6.763635	-0.068845	3.443768
361.197663	4045.044803	6.768640	-0.068996	3.447136
361.002848	4053.114732	6.773645	-0.068965	3.450484
361.448715	4061.154198	6.778650	-0.069053	3.453837
362.229251	4069.123129	6.783654	-0.069204	3.457169
362.400921	4077.156567	6.788659	-0.069241	3.460504
362.384528	4085.230496	6.793664	-0.069243	3.463846
362.566815	4093.262112	6.798669	-0.069282	3.467174
363.501692	4101.214138	6.803674	-0.069462	3.470491
363.925000	4109.261698	6.808678	-0.069546	3.473827
363.940235	4117.303883	6.813683	-0.069554	3.477145
364.324467	4125.333196	6.818688	-0.069631	3.480465
364.419054	4133.338956	6.823693	-0.069653	3.483764
365.337753	4141.287186	6.828698	-0.069830	3.487063
365.779980	4149.363514	6.833702	-0.069917	3.490395
365.853663	4157.436017	6.838707	-0.069936	3.493711
366.095728	4165.521903	6.843712	-0.069986	3.497034
366.748187	4173.451182	6.848717	-0.070113	3.500303
366.811258	4181.561449	6.853722	-0.070130	3.503624
367.058409	4189.631325	6.858726	-0.070181	3.506932
366.792413	4197.708760	6.863731	-0.070137	3.510223
367.271685	4205.687756	6.868736	-0.070232	3.513494
367.716040	4213.650335	6.873741	-0.070319	3.516755
368.137500	4221.664478	6.878746	-0.070403	3.520033
368.877495	4229.599327	6.883750	-0.070546	3.523285
369.353114	4237.633834	6.888755	-0.070640	3.526567
369.939077	4245.662123	6.893760	-0.070754	3.529846
369.945763	4253.789090	6.898765	-0.070761	3.533144
370.249886	4261.816765	6.903770	-0.070823	3.536408
370.831532	4269.790575	6.908774	-0.070936	3.539656
370.945688	4277.834066	6.913779	-0.070963	3.542915
371.492861	4285.851910	6.918784	-0.071070	3.546173
372.409214	4293.781954	6.923789	-0.071245	3.549404
372.538233	4301.935127	6.928794	-0.071275	3.552698
372.536466	4310.044653	6.933798	-0.071280	3.555968
372.948185	4317.952776	6.938803	-0.071361	3.559165
373.652437	4325.919860	6.943808	-0.071498	3.562393
373.713427	4333.980996	6.948813	-0.071514	3.565636
373.960418	4342.029318	6.953818	-0.071566	3.568876
374.218204	4350.092049	6.958822	-0.071619	3.572120
373.806312	4358.191228	6.963827	-0.071547	3.575355
374.074813	4366.201643	6.968832	-0.071603	3.578572
374.706667	4374.119815	6.973837	-0.071725	3.581759
374.699961	4382.180931	6.978842	-0.071729	3.584983
375.127897	4390.193721	6.983846	-0.071814	3.588196
375.531978	4398.232872	6.988851	-0.071895	3.591417
376.047236	4406.214864	6.993856	-0.071996	3.594615
376.653424	4414.160693	6.998861	-0.072114	3.597799
377.053134	4422.281166	7.003866	-0.072194	3.601043
377.407330	4430.246760	7.008870	-0.072265	3.604221
377.387800	4438.348928	7.013875	-0.072266	3.607440
378.184710	4446.325143	7.018880	-0.072420	3.610629
378.295748	4454.383604	7.023885	-0.072446	3.613829
378.922568	4462.400225	7.028890	-0.072568	3.617023
379.126957	4470.427013	7.033894	-0.072611	3.620207
379.239564	4478.471501	7.038899	-0.072637	3.623393
379.804221	4486.493936	7.043904	-0.072748	3.626579
380.731834	4494.402868	7.048909	-0.072925	3.629728
381.449758	4502.453566	7.053914	-0.073064	3.632925
381.244793	4510.608887	7.058918	-0.073032	3.636133
381.541145	4518.543912	7.063923	-0.073092	3.639267
381.884499	4526.605636	7.068928	-0.073161	3.642448
381.680870	4534.663814	7.073933	-0.073128	3.645611
382.274020	4542.644349	7.078938	-0.073244	3.648762
383.538709	4550.581073	7.083942	-0.073485	3.651911
383.514504	4558.694053	7.088947	-0.073485	3.655092
383.775791	4566.751969	7.093952	-0.073539	3.658255
383.684791	4574.787175	7.098957	-0.073528	3.661398
383.925764	4582.803079	7.103962	-0.073578	3.664539
384.696615	4590.784611	7.108966	-0.073726	3.667679
384.911654	4598.814786	7.113971	-0.073772	3.670820
385.042097	4606.890579	7.118976	-0.073801	3.673973
385.137743	4614.938090	7.123981	-0.073824	3.677112
385.696933	4622.898334	7.128986	-0.073933	3.680226
385.752550	4630.937571	7.133990	-0.073949	3.683356
386.140594	4638.925771	7.138995	-0.074027	3.686471
386.779369	4646.924857	7.144000	-0.074151	3.689595
386.634210	4654.991940	7.149005	-0.074129	3.692721
387.447120	4662.985258	7.154010	-0.074285	3.695842
388.024538	4670.984563	7.159014	-0.074398	3.698956
387.847562	4679.107482	7.164019	-0.074370	3.702095
388.198346	4687.119664	7.169024	-0.074441	3.705203
388.772303	4695.097229	7.174029	-0.074553	3.708300
389.159941	4703.179019	7.179034	-0.074630	3.711430
388.999852	4711.274854	7.184038	-0.074606	3.714549
389.612062	4719.199326	7.189043	-0.074725	3.717619
389.921661	4727.286757	7.194048	-0.074788	3.720741
390.103089	4735.204449	7.199053	-0.074827	3.723792
390.143672	4743.287397	7.204058	-0.074840	3.726901
390.670256	4751.282061	7.209062	-0.074943	3.729985
391.099488	4759.261421	7.214067	-0.075028	3.733059
391.623071	4767.312305	7.219072	-0.075131	3.736159
391.646933	4775.322472	7.224077	-0.075140	3.739229
392.358403	4783.330911	7.229082	-0.075278	3.742312
392.778836	4791.331465	7.234086	-0.075362	3.745383
392.954266	4799.398564	7.239091	-0.075400	3.748471
392.756177	4807.520738	7.244096	-0.075368	3.751568
392.687240	4815.509559	7.249101	-0.075360	3.754615
392.974613	4823.524875	7.254106	-0.075419	3.757678
393.404841	4831.526368	7.259110	-0.075504	3.760736
393.789891	4839.479159	7.264115	-0.075581	3.763773
393.937921	4847.567566	7.269120	-0.075614	3.766853
394.225058	4855.545478	7.274125	-0.075673	3.769891
394.808601	4863.569055	7.279130	-0.075786	3.772952
394.820108	4871.688479	7.284134	-0.075794	3.776033
395.019311	4879.632372	7.289139	-0.075836	3.779049
395.885416	4887.629738	7.294144	-0.076003	3.782098
396.294489	4895.620003	7.299149	-0.076084	3.785132
396.812415	4903.677907	7.304154	-0.076186	3.788191
397.019816	4911.764866	7.309158	-0.076230	3.791252
397.401560	4919.688995	7.314163	-0.076306	3.794252
397.362138	4927.815721	7.319168	-0.076304	3.797317
397.736139	4935.796352	7.324173	-0.076379	3.800334
398.079707	4943.789479	7.329178	-0.076448	3.803352
398.109458	4951.876058	7.334182	-0.076458	3.806396
398.118214	4959.898130	7.339187	-0.076465	3.809413
399.025911	4967.898576	7.344192	-0.076640	3.812440
399.170524	4975.908015	7.349197	-0.076672	3.815450
399.423685	4983.922395	7.354202	-0.076724	3.818462
399.639550	4991.986258	7.359206	-0.076769	3.821489
399.612117	5000.010939	7.364211	-0.076770	3.824494
400.012763	5008.058469	7.369216	-0.076849	3.827515
400.092861	5016.072033	7.374221	-0.076870	3.830513
400.642504	5024.057792	7.379226	-0.076977	3.833509
401.209806	5032.065746	7.384230	-0.077088	3.836511
401.356145	5040.061129	7.389235	-0.077120	3.839497
402.017200	5048.124358	7.394240	-0.077249	3.842517
401.798902	5056.189581	7.399245	-0.077213	3.845516
402.229505	5064.211141	7.404250	-0.077299	3.848511
402.490389	5072.234584	7.409254	-0.077352	3.851500
403.297596	5080.135706	7.414259	-0.077508	3.854453
403.706348	5088.195444	7.419264	-0.077589	3.857454
404.107339	5096.234304	7.424269	-0.077669	3.860445
404.516691	5104.249621	7.429274	-0.077751	3.863425
404.733609	5112.297319	7.434278	-0.077796	3.866411
404.885310	5120.287491	7.439283	-0.077830	3.869371
405.594821	5128.406374	7.444288	-0.077967	3.872389
405.841858	5136.456246	7.449293	-0.078018	3.875369
406.159518	5144.411245	7.454298	-0.078083	3.878313
406.394527	5152.447257	7.459302	-0.078132	3.881283
406.822226	5160.362865	7.464307	-0.078216	3.884210
407.100991	5168.419971	7.469312	-0.078273	3.887184
407.252515	5176.460644	7.474317	-0.078307	3.890147
407.659765	5184.463015	7.479322	-0.078388	3.893099
407.958123	5192.558277	7.484326	-0.078449	3.896080
408.289925	5200.454835	7.489331	-0.078516	3.898987
408.791268	5208.520191	7.494336	-0.078614	3.901957
409.225984	5216.444755	7.499341	-0.078700	3.904872
409.219940	5224.563523	7.504346	-0.078704	3.907847
409.307639	5232.673246	7.509350	-0.078726	3.910818
409.750419	5240.614104	7.514355	-0.078814	3.913732
410.049039	5248.672073	7.519360	-0.078875	3.916684
410.398105	5256.636139	7.524365	-0.078945	3.919600
410.835857	5264.688896	7.529370	-0.079031	3.922549
411.173496	5272.691504	7.534374	-0.079100	3.925474
411.693647	5280.645302	7.539379	-0.079202	3.928383
412.130684	5288.745027	7.544384	-0.079288	3.931342
412.662268	5296.710570	7.549389	-0.079392	3.934251
412.700305	5304.795293	7.554394	-0.079405	3.937192
412.513149	5312.892498	7.559398	-0.079375	3.940131
412.871645	5320.834438	7.564403	-0.079447	3.943021
413.049629	5328.912929	7.569408	-0.079485	3.945956
413.566228	5336.893322	7.574413	-0.079587	3.948859
414.194389	5344.931065	7.579418	-0.079709	3.951783
414.551008	5352.915398	7.584422	-0.079781	3.954680
415.075213	5360.908555	7.589427	-0.079883	3.957581
415.834848	5368.890853	7.594432	-0.080030	3.960481
415.946117	5376.950532	7.599437	-0.080056	3.963394
415.921070	5385.027286	7.604442	-0.080057	3.966309
415.911118	5393.065073	7.609446	-0.080060	3.969208
416.409523	5401.026531	7.614451	-0.080158	3.972087
416.514615	5409.114718	7.619456	-0.080183	3.975002
416.621666	5417.129833	7.624461	-0.080208	3.977889
417.265387	5425.108223	7.629466	-0.080333	3.980769
417.516237	5433.109096	7.634470	-0.080385	3.983649
417.883621	5441.086769	7.639475	-0.080458	3.986520
418.214112	5449.133051	7.644480	-0.080525	3.989413
418.148472	5457.250437	7.649485	-0.080518	3.992323
418.231834	5465.267264	7.654490	-0.080539	3.995197
419.085403	5473.193171	7.659494	-0.080703	3.998050
419.228650	5481.248582	7.664499	-0.080735	4.000935
419.798288	5489.195471	7.669504	-0.080846	4.003786
420.003999	5497.218650	7.674509	-0.080890	4.006656
420.283681	5505.275716	7.679514	-0.080947	4.009537
421.016828	5513.310624	7.684518	-0.081089	4.012416
421.164993	5521.330515	7.689523	-0.081122	4.015277
421.686658	5529.345998	7.694528	-0.081224	4.018141
421.860829	5537.398288	7.699533	-0.081262	4.021011
422.603426	5545.323332	7.704538	-0.081405	4.023842
422.583439	5553.458534	7.709542	-0.081407	4.026734
423.177371	5561.388022	7.714547	-0.081522	4.029560
423.722372	5569.472472	7.719552	-0.081629	4.032439
423.854946	5577.493412	7.724557	-0.081659	4.035286
423.927208	5585.567712	7.729562	-0.081678	4.038149
424.281162	5593.594683	7.734566	-0.081749	4.040998
424.420253	5601.527588	7.739571	-0.081780	4.043808
425.219837	5609.533175	7.744576	-0.081934	4.046652
425.703806	5617.525027	7.749581	-0.082029	4.049484
425.818951	5625.607783	7.754586	-0.082056	4.052341
426.224375	5633.607565	7.759590	-0.082137	4.055171
426.775372	5641.603263	7.764595	-0.082244	4.057999
426.807309	5649.701604	7.769600	-0.082256	4.060854
426.853830	5657.667595	7.774605	-0.082269	4.063661
427.498844	5665.703156	7.779610	-0.082395	4.066498
427.998651	5673.750790	7.784614	-0.082493	4.069336
427.955844	5681.804137	7.789619	-0.082490	4.072166
428.121698	5689.830270	7.794624	-0.082526	4.074987
428.361834	5697.801086	7.799629	-0.082576	4.077789
428.378562	5705.873195	7.804634	-0.082585	4.080620
428.372437	5713.865441	7.809638	-0.082589	4.083421
428.660341	5721.893814	7.814643	-0.082648	4.086237
429.140037	5729.841430	7.819648	-0.082742	4.089026
429.437652	5737.924474	7.824653	-0.082803	4.091857
429.851979	5745.895900	7.829658	-0.082885	4.094649
429.957171	5753.992799	7.834662	-0.082910	4.097478
430.064474	5761.935986	7.839667	-0.082935	4.100252
430.975326	5769.932884	7.844672	-0.083110	4.103054
431.180262	5777.975529	7.849677	-0.083153	4.105860
431.636937	5785.988641	7.854682	-0.083243	4.108658
432.032033	5794.057407	7.859686	-0.083322	4.111472
432.004533	5802.041682	7.864691	-0.083322	4.114248
432.621351	5810.026739	7.869696	-0.083442	4.117032
432.792508	5818.042052	7.874701	-0.083479	4.119819
432.868197	5826.102567	7.879706	-0.083499	4.122617
433.247549	5834.096542	7.884710	-0.083575	4.125395
433.099749	5842.124443	7.889715	-0.083552	4.128176
434.367259	5850.071119	7.894720	-0.083793	4.130946
434.526023	5858.131709	7.899725	-0.083828	4.133738
434.878269	5866.227516	7.904730	-0.083899	4.136543
435.085385	5874.208860	7.909734	-0.083943	4.139305
435.609958	5882.209049	7.914739	-0.084046	4.142075
436.135325	5890.199411	7.919744	-0.084149	4.144840
436.181461	5898.252929	7.924749	-0.084163	4.147619
436.716162	5906.241321	7.929754	-0.084267	4.150380
436.810104	5914.333917	7.934758	-0.084290	4.153169
437.398680	5922.304197	7.939763	-0.084405	4.155921
437.454070	5930.348370	7.944768	-0.084420	4.158689
437.716168	5938.376850	7.949773	-0.084474	4.161453
438.208922	5946.298885	7.954778	-0.084571	4.164181
438.585185	5954.404210	7.959782	-0.084647	4.166968
438.816145	5962.361913	7.964787	-0.084695	4.169702
438.990067	5970.478142	7.969792	-0.084732	4.172487
439.032180	5978.483287	7.974797	-0.084746	4.175230
439.192679	5986.482293	7.979802	-0.084781	4.177971
439.607012	5994.534395	7.984806	-0.084863	4.180732
439.354920	6002.553817	7.989811	-0.084821	4.183471
440.127615	6010.524950	7.994816	-0.084970	4.186205
439.682460	6018.629134	7.999821	-0.084893	4.188967
440.130162	6026.653296	8.004826	-0.084981	4.191711
440.401821	6034.704412	8.009830	-0.085037	4.194461
441.060168	6042.605947	8.014835	-0.085165	4.197161
441.486292	6050.612274	8.019840	-0.085249	4.199894
441.340239	6058.650303	8.024845	-0.085227	4.202628
441.704610	6066.635383	8.029850	-0.085300	4.205349
441.982363	6074.712224	8.034854	-0.085357	4.208098
441.494428	6082.823077	8.039859	-0.085272	4.210848
442.297834	6090.747312	8.044864	-0.085427	4.213547
442.544862	6098.785066	8.049869	-0.085478	4.216277
442.939653	6106.716573	8.054874	-0.085556	4.218971
442.547634	6114.834078	8.059878	-0.085489	4.221717
442.752220	6122.782015	8.064883	-0.085532	4.224411
443.560241	6130.839834	8.069888	-0.085688	4.227146
443.795395	6138.841667	8.074893	-0.085737	4.229855
444.059090	6146.833063	8.079898	-0.085791	4.232558
444.063469	6154.900546	8.084902	-0.085797	4.235283
444.693054	6162.831044	8.089907	-0.085919	4.237967
444.907683	6170.903513	8.094912	-0.085965	4.240692
444.605404	6178.935743	8.099917	-0.085914	4.243396
445.129521	6186.938904	8.104922	-0.086016	4.246098
445.307445	6194.959564	8.109926	-0.086055	4.248800
446.054518	6202.915640	8.114931	-0.086199	4.251484
446.117302	6210.988220	8.119936	-0.086216	4.254199
446.546841	6219.021809	8.124941	-0.086301	4.256903
446.636809	6227.007309	8.129946	-0.086323	4.259585
447.184764	6235.041444	8.134950	-0.086430	4.262287
447.592608	6242.986214	8.139955	-0.086511	4.264955
447.301189	6251.178726	8.144960	-0.086462	4.267698
447.329752	6259.163162	8.149965	-0.086473	4.270373
447.759499	6267.107779	8.154970	-0.086558	4.273036
448.298191	6275.168395	8.159974	-0.086664	4.275738
448.659225	6283.103797	8.164979	-0.086736	4.278394
449.219679	6291.129478	8.169984	-0.086846	4.281080
449.266978	6299.150114	8.174989	-0.086860	4.283759
448.669261	6307.279369	8.179994	-0.086754	4.286466
449.336367	6315.193153	8.184998	-0.086883	4.289111
449.599645	6323.258761	8.190003	-0.086937	4.291801
449.780370	6331.242648	8.195008	-0.086976	4.294461
449.400956	6339.381413	8.200013	-0.086911	4.297167
449.402518	6347.370628	8.205018	-0.086916	4.299824
449.755070	6355.394217	8.210022	-0.086987	4.302495
449.586512	6363.349857	8.215027	-0.086961	4.305136
450.421063	6371.343042	8.220032	-0.087121	4.307797
450.263312	6379.444766	8.225037	-0.087097	4.310484
450.600152	6387.406265	8.230042	-0.087165	4.313127
450.922966	6395.423087	8.235046	-0.087231	4.315786
451.513221	6403.332762	8.240051	-0.087346	4.318410
452.151536	6411.358601	8.245056	-0.087470	4.321072
451.589477	6419.404714	8.250061	-0.087370	4.323729
452.121936	6427.449908	8.255066	-0.087475	4.326392
452.282717	6435.473265	8.260070	-0.087510	4.329044
452.529591	6443.494840	8.265075	-0.087561	4.331694
453.021409	6451.459819	8.270080	-0.087658	4.334326
453.528973	6459.461679	8.275085	-0.087757	4.336969
453.322877	6467.528760	8.280090	-0.087724	4.339626
453.525841	6475.580881	8.285094	-0.087767	4.342279
453.996605	6483.498130	8.290099	-0.087860	4.344888
454.255862	6491.604553	8.295104	-0.087914	4.347557
454.562118	6499.606715	8.300109	-0.087976	4.350190
454.522843	6507.721337	8.305114	-0.087974	4.352855
455.448252	6515.683690	8.310118	-0.088151	4.355476
455.173470	6523.704028	8.315123	-0.088105	4.358106
455.171314	6531.797502	8.320128	-0.088110	4.360760
455.574440	6539.668064	8.325133	-0.088190	4.363342
455.573166	6547.718898	8.330138	-0.088195	4.365979
455.838116	6555.726076	8.335142	-0.088250	4.368602
456.320227	6563.709793	8.340147	-0.088345	4.371217
456.875023	6571.735204	8.345152	-0.088453	4.373844
456.719132	6579.814599	8.350157	-0.088430	4.376483
456.966168	6587.774938	8.355162	-0.088481	4.379084
457.486122	6595.815034	8.360166	-0.088583	4.381711
457.435543	6603.791059	8.365171	-0.088579	4.384312
457.407787	6611.938072	8.370176	-0.088579	4.386967
457.865150	6619.851451	8.375181	-0.088669	4.389548
458.334622	6627.883598	8.380186	-0.088762	4.392165
458.502395	6635.914965	8.385190	-0.088798	4.394780
458.731103	6643.917385	8.390195	-0.088846	4.397383
458.499259	6652.035112	8.395200	-0.088808	4.400020
458.453772	6660.098408	8.400205	-0.088805	4.402638
458.885950	6667.976876	8.405210	-0.088890	4.405198
459.479653	6676.009297	8.410214	-0.089006	4.407807
459.835295	6684.018228	8.415219	-0.089078	4.410405
459.513055	6692.169331	8.420224	-0.089023	4.413044
460.206013	6700.122254	8.425229	-0.089157	4.415623
460.184388	6708.119493	8.430234	-0.089158	4.418211
460.684716	6716.182983	8.435238	-0.089257	4.420822
460.313351	6724.222706	8.440243	-0.089193	4.423418
461.629132	6732.135376	8.445248	-0.089443	4.425981
461.814682	6740.162761	8.450253	-0.089483	4.428574
461.366975	6748.262370	8.455258	-0.089405	4.431185
462.046088	6756.278689	8.460262	-0.089536	4.433773
461.877624	6764.312501	8.465267	-0.089510	4.436362
462.020331	6772.245210	8.470272	-0.089542	4.438917
462.384904	6780.307171	8.475277	-0.089615	4.441514
463.004721	6788.213797	8.480282	-0.089735	4.444061
463.028757	6796.383866	8.485286	-0.089745	4.446688
463.340128	6804.301794	8.490291	-0.089808	4.449233
463.714433	6812.382944	8.495296	-0.089883	4.451830
463.495941	6820.443542	8.500301	-0.089848	4.454416
463.151550	6828.486212	8.505306	-0.089789	4.456994
463.778013	6836.425162	8.510310	-0.089911	4.459542
464.165144	6844.434636	8.515315	-0.089988	4.462110
464.145053	6852.412556	8.520320	-0.089989	4.464664
464.480758	6860.488776	8.525325	-0.090057	4.467250
464.753016	6868.443729	8.530330	-0.090113	4.469796
465.303896	6876.495405	8.535334	-0.090221	4.472372
464.786950	6884.526721	8.540339	-0.090130	4.474935
464.919640	6892.566845	8.545344	-0.090160	4.477503
465.263215	6900.550266	8.550349	-0.090229	4.480051
465.826567	6908.541526	8.555354	-0.090339	4.482602
466.218996	6916.519079	8.560359	-0.090417	4.485146
466.194072	6924.590655	8.565363	-0.090418	4.487717
466.630233	6932.603530	8.570368	-0.090504	4.490270
466.779645	6940.626442	8.575373	-0.090537	4.492823
467.061873	6948.607290	8.580378	-0.090595	4.495362
467.756240	6956.606812	8.585383	-0.090730	4.497906
467.691983	6964.628367	8.590387	-0.090723	4.500454
467.761809	6972.710056	8.595392	-0.090741	4.503020
468.240852	6980.657179	8.600397	-0.090835	4.505543
468.349096	6988.705408	8.605402	-0.090861	4.508095
468.730059	6996.755453	8.610407	-0.090937	4.510647
468.608261	7004.779775	8.615411	-0.090920	4.513188
468.867549	7012.727866	8.620416	-0.090973	4.515705
468.730081	7020.768244	8.625421	-0.090953	4.518248
469.580643	7028.752386	8.630426	-0.091116	4.520775
469.837254	7036.746850	8.635431	-0.091169	4.523302
469.788640	7044.790194	8.640435	-0.091165	4.525842
470.239903	7052.799966	8.645440	-0.091255	4.528371
470.158021	7060.902191	8.650445	-0.091245	4.530927
469.669523	7068.904453	8.655450	-0.091159	4.533449
470.518723	7076.903850	8.660455	-0.091322	4.535971
470.923040	7084.823393	8.665459	-0.091403	4.538467
470.903140	7092.956196	8.670464	-0.091404	4.541026
470.796496	7100.917549	8.675469	-0.091389	4.543530
471.594363	7108.882421	8.680474	-0.091543	4.546037
471.934881	7116.915984	8.685479	-0.091612	4.548562
471.779572	7124.978567	8.690483	-0.091588	4.551093
472.303139	7132.944371	8.695488	-0.091691	4.553595
472.237142	7141.074040	8.700493	-0.091684	4.556145
472.511122	7148.926124	8.705498	-0.091740	4.558607
472.127783	7157.123596	8.710503	-0.091674	4.561175
472.316034	7165.022875	8.715507	-0.091714	4.563649
472.411167	7173.104672	8.720512	-0.091737	4.566179
472.909453	7181.092840	8.725517	-0.091835	4.568679
472.719444	7189.174316	8.730522	-0.091805	4.571205
473.083295	7197.113310	8.735527	-0.091878	4.573686
473.194091	7205.151070	8.740531	-0.091904	4.576197
473.259985	7213.173508	8.745536	-0.091921	4.578701
473.936235	7221.169425	8.750541	-0.092052	4.581196
473.863640	7229.118319	8.755546	-0.092044	4.583674
473.936559	7237.244228	8.760551	-0.092063	4.586207
474.039555	7245.205081	8.765555	-0.092087	4.588686
474.148316	7253.270589	8.770560	-0.092113	4.591197
474.325916	7261.248956	8.775565	-0.092151	4.593679
474.765156	7269.235792	8.780570	-0.092238	4.596163
475.162979	7277.229280	8.785575	-0.092317	4.598648
475.464550	7285.222537	8.790579	-0.092378	4.601131
475.774469	7293.180977	8.795584	-0.092441	4.603601
475.925216	7301.331492	8.800589	-0.092475	4.606130
476.497333	7309.213525	8.805594	-0.092586	4.608575
476.187406	7317.439686	8.810599	-0.092534	4.611124
476.645721	7325.335854	8.815603	-0.092624	4.613570
477.079084	7333.399870	8.820608	-0.092710	4.616066
477.097976	7341.348076	8.825613	-0.092719	4.618526
477.599807	7349.356288	8.830618	-0.092818	4.621002
477.930768	7357.335905	8.835623	-0.092885	4.623469
477.798415	7365.426654	8.840627	-0.092865	4.625968
478.003468	7373.465743	8.845632	-0.092909	4.628450
478.318385	7381.523309	8.850637	-0.092972	4.630936
478.750296	7389.433367	8.855642	-0.093058	4.633376
478.949690	7397.532274	8.860647	-0.093100	4.635872
479.348986	7405.464260	8.865651	-0.093180	4.638316
479.069281	7413.618711	8.870656	-0.093133	4.640826
478.981619	7421.530904	8.875661	-0.093122	4.643261
479.070900	7429.563024	8.880666	-0.093144	4.645732
479.298081	7437.582262	8.885671	-0.093191	4.648197
479.734346	7445.580589	8.890675	-0.093278	4.650654
479.528521	7453.600039	8.895680	-0.093245	4.653117
480.052830	7461.623442	8.900685	-0.093347	4.655579
480.244883	7469.619319	8.905690	-0.093388	4.658032
480.295116	7477.699751	8.910695	-0.093403	4.660509
480.888358	7485.624398	8.915699	-0.093519	4.662937
481.313841	7493.664243	8.920704	-0.093603	4.665399
481.267444	7501.717736	8.925709	-0.093600	4.667864
481.435678	7509.752484	8.930714	-0.093636	4.670322
482.033851	7517.809959	8.935719	-0.093753	4.672785
481.591319	7525.838505	8.940723	-0.093676	4.675239
482.184569	7533.760574	8.945728	-0.093791	4.677659
482.043973	7541.796245	8.950733	-0.093770	4.680112
482.472155	7549.783686	8.955738	-0.093855	4.682549
482.486784	7557.782231	8.960743	-0.093863	4.684988
482.871589	7565.782205	8.965747	-0.093940	4.687426
483.099739	7573.839206	8.970752	-0.093988	4.689880
483.218453	7581.875469	8.975757	-0.094015	4.692327
483.317588	7589.831751	8.980762	-0.094039	4.694748
483.552896	7597.924206	8.985767	-0.094088	4.697209
483.719193	7605.868654	8.990771	-0.094124	4.699624
483.814800	7614.024532	8.995776	-0.094147	4.702102
483.960055	7621.917642	9.000781	-0.094179	4.704498
484.295587	7629.953695	9.005786	-0.094247	4.706937
484.438713	7637.961104	9.010791	-0.094279	4.709366
484.982182	7645.989368	9.015795	-0.094385	4.711799
485.069477	7653.975051	9.020800	-0.094407	4.714219
484.934169	7662.071803	9.025805	-0.094387	4.716672
484.966801	7670.001495	9.030810	-0.094398	4.719072
485.203854	7678.164635	9.035815	-0.094447	4.721542
485.311512	7686.035971	9.040819	-0.094472	4.723922
485.585474	7694.118044	9.045824	-0.094529	4.726364
486.180699	7702.059865	9.050829	-0.094645	4.728762
486.215462	7710.129154	9.055834	-0.094656	4.731199
486.682660	7718.121987	9.060839	-0.094749	4.733610
486.725308	7726.154186	9.065843	-0.094762	4.736033
486.680997	7734.210566	9.070848	-0.094759	4.738461
486.804171	7742.259964	9.075853	-0.094787	4.740887
486.684411	7750.315710	9.080858	-0.094770	4.743313
486.667904	7758.302746	9.085863	-0.094772	4.745717
486.889495	7766.257458	9.090867	-0.094818	4.748110
487.622313	7774.289271	9.095872	-0.094960	4.750523
487.640049	7782.342985	9.100877	-0.094969	4.752944
488.023126	7790.298111	9.105882	-0.095045	4.755332
488.158770	7798.317495	9.110887	-0.095076	4.757740
488.097213	7806.391160	9.115891	-0.095069	4.760163
489.105277	7814.256485	9.120896	-0.095262	4.762519
489.053176	7822.322909	9.125901	-0.095258	4.764937
488.905080	7830.375774	9.130906	-0.095235	4.767351
489.181399	7838.457891	9.135911	-0.095292	4.769770
489.395412	7846.392297	9.140915	-0.095337	4.772144
489.738273	7854.444851	9.145920	-0.095406	4.774552
489.574615	7862.512814	9.150925	-0.095381	4.776965
489.333218	7870.485723	9.155930	-0.095341	4.779349
490.199614	7878.482319	9.160935	-0.095508	4.781735
489.754411	7886.450444	9.165939	-0.095430	4.784115
490.574434	7894.507227	9.170944	-0.095588	4.786517
490.557410	7902.552182	9.175949	-0.095590	4.788916
490.872801	7910.533945	9.180954	-0.095654	4.791295
491.085947	7918.536369	9.185959	-0.095699	4.793678
490.876321	7926.608912	9.190963	-0.095665	4.796083
490.887523	7934.583313	9.195968	-0.095672	4.798457
491.574883	7942.578742	9.200973	-0.095805	4.800833
492.003736	7950.554036	9.205978	-0.095890	4.803203
492.218053	7958.581038	9.210983	-0.095936	4.805588
492.573188	7966.615059	9.215987	-0.096007	4.807973
492.775468	7974.653236	9.220992	-0.096050	4.810359
493.129914	7982.674441	9.225997	-0.096121	4.812738
493.196220	7990.099849	9.231002	-0.096138	4.814940
493.318721	7994.793371	9.236007	-0.096164	4.816331

493.793370	7997.319238	9.241011	-0.096254	4.817078
493.736252	7998.735106	9.246016	-0.096244	4.817498
493.366159	7999.240722	9.251021	-0.096176	4.817650
493.473776	7999.982783	9.256026	-0.096196	4.817869
494.039537	7999.980299	9.261031	-0.096302	4.817866
493.568525	7999.992556	9.266035	-0.096214	4.817872
493.717873	7999.994680	9.271040	-0.096242	4.817872
494.438672	8000.008099	9.276045	-0.096376	4.817872
494.137158	7999.946921	9.281050	-0.096320	4.817856
494.573020	7999.976300	9.286055	-0.096401	4.817862
494.806135	7999.968030	9.291059	-0.096444	4.817859
493.744888	8000.096188	9.296064	-0.096247	4.817901
493.959057	8000.066579	9.301069	-0.096287	4.817892
494.199519	8000.084749	9.306074	-0.096331	4.817896
494.627220	8000.065555	9.311079	-0.096411	4.817889
494.523570	8000.030368	9.316083	-0.096392	4.817879
494.767759	8000.031737	9.321088	-0.096437	4.817878
494.685059	8000.059001	9.326093	-0.096422	4.817886
494.928651	7999.976086	9.331098	-0.096467	4.817861
495.111917	7999.988176	9.336103	-0.096501	4.817864
494.887258	7999.990243	9.341107	-0.096459	4.817865
495.065446	8000.001207	9.346112	-0.096492	4.817868
494.777102	8000.024489	9.351117	-0.096439	4.817876
495.312215	8000.005772	9.356122	-0.096538	4.817868
495.128820	8000.074795	9.361127	-0.096504	4.817889
494.477023	8000.091848	9.366131	-0.096383	4.817897
494.947382	8000.115400	9.371136	-0.096470	4.817902
494.558374	8000.111966	9.376141	-0.096398	4.817903
494.909403	8000.067451	9.381146	-0.096463	4.817888
494.597185	8000.130425	9.386151	-0.096405	4.817908
495.045423	8000.082028	9.391155	-0.096489	4.817892
494.985091	8000.095916	9.396160	-0.096477	4.817896
494.624910	8000.089732	9.401165	-0.096410	4.817896
494.510293	8000.089152	9.406170	-0.096389	4.817896
495.128126	8000.104271	9.411175	-0.096504	4.817898
494.938831	8000.137391	9.416179	-0.096469	4.817909
495.331248	8000.109269	9.421184	-0.096542	4.817899
495.212169	8000.095983	9.426189	-0.096520	4.817895
495.239215	8000.040534	9.431194	-0.096525	4.817879
495.107805	8000.092388	9.436199	-0.096500	4.817895
495.152495	8000.070900	9.441203	-0.096508	4.817888
495.643959	8000.037868	9.446208	-0.096600	4.817876
495.541600	8000.068013	9.451213	-0.096581	4.817886
495.479903	8000.052384	9.456218	-0.096569	4.817881
495.471491	8000.097563	9.461223	-0.096568	4.817895
495.556959	8000.087191	9.466227	-0.096584	4.817891
495.699044	8000.113444	9.471232	-0.096610	4.817898
495.940112	8000.123199	9.476237	-0.096655	4.817900
495.967220	8000.035091	9.481242	-0.096660	4.817874
495.884483	8000.072890	9.486247	-0.096645	4.817886
496.060819	8000.029049	9.491251	-0.096677	4.817872
495.983912	8000.062716	9.496256	-0.096663	4.817882
495.939098	8000.044168	9.501261	-0.096655	4.817877
495.715376	8000.077851	9.506266	-0.096613	4.817888
496.169244	8000.052712	9.511271	-0.096697	4.817878
495.457233	8000.102615	9.516275	-0.096565	4.817896
495.769205	8000.123914	9.521280	-0.096623	4.817901
495.851363	8000.071356	9.526285	-0.096638	4.817885
495.634600	8000.077748	9.531290	-0.096598	4.817888
495.767732	8000.087018	9.536295	-0.096623	4.817890
495.833578	8000.068992	9.541299	-0.096635	4.817885
496.336533	8000.076158	9.546304	-0.096729	4.817885
496.507410	8000.050148	9.551309	-0.096760	4.817876
496.458912	8000.006263	9.556314	-0.096751	4.817863
496.918233	8000.054948	9.561319	-0.096837	4.817876
497.001467	7999.993977	9.566323	-0.096852	4.817857
496.733337	8000.020705	9.571328	-0.096802	4.817867
496.567267	8000.049942	9.576333	-0.096771	4.817876
497.292902	7999.939131	9.581338	-0.096906	4.817840
496.549811	8000.006498	9.586343	-0.096768	4.817863
497.211738	7999.953775	9.591347	-0.096891	4.817845
497.310414	7999.972036	9.596352	-0.096910	4.817850
497.097848	7999.992182	9.601357	-0.096870	4.817857
496.650111	8000.016351	9.606362	-0.096787	4.817866
496.610017	8000.086363	9.611367	-0.096779	4.817886
496.722132	8000.037392	9.616371	-0.096800	4.817872
496.492676	8000.062565	9.621376	-0.096757	4.817880
496.705226	8000.061379	9.626381	-0.096797	4.817879
496.654263	8000.033261	9.631386	-0.096787	4.817871
496.409050	8000.099295	9.636391	-0.096742	4.817891
496.624258	8000.057061	9.641395	-0.096782	4.817878
496.427256	8000.061627	9.646400	-0.096745	4.817880
497.160144	7999.959347	9.651405	-0.096882	4.817847
497.411139	7999.872322	9.656410	-0.096928	4.817820
497.383270	7999.997291	9.661415	-0.096923	4.817857
497.494357	7999.957787	9.666419	-0.096944	4.817845
497.397037	7999.940596	9.671424	-0.096926	4.817840
497.384073	8000.028905	9.676429	-0.096923	4.817866
497.374404	7999.939218	9.681434	-0.096921	4.817840
497.641830	7999.902995	9.686439	-0.096971	4.817828
497.240259	7999.971015	9.691443	-0.096896	4.817850
497.199900	7999.996777	9.696448	-0.096889	4.817857
496.953985	8000.023822	9.701453	-0.096843	4.817867
497.148551	7999.921244	9.706458	-0.096879	4.817835
497.381658	7999.989883	9.711463	-0.096923	4.817855
497.534794	7999.927801	9.716467	-0.096951	4.817836
497.311073	7999.976232	9.721472	-0.096909	4.817851
497.217131	8000.011765	9.726477	-0.096892	4.817862
496.989627	8000.003253	9.731482	-0.096850	4.817860
496.731535	8000.051195	9.736487	-0.096802	4.817876
497.098884	7999.999541	9.741491	-0.096870	4.817859
497.052094	8000.066297	9.746496	-0.096861	4.817879
496.973262	8000.051476	9.751501	-0.096846	4.817875
497.102053	7999.998529	9.756506	-0.096870	4.817858
497.392851	8000.021637	9.761511	-0.096925	4.817864
497.454005	7999.951922	9.766515	-0.096936	4.817843
497.415874	7999.999839	9.771520	-0.096929	4.817857
497.380975	8000.007768	9.776525	-0.096922	4.817860
497.347437	7999.986219	9.781530	-0.096916	4.817854
497.161735	8000.115259	9.786535	-0.096882	4.817893
497.962118	7999.935984	9.791539	-0.097030	4.817836
497.800786	7999.958967	9.796544	-0.097000	4.817844
497.851163	8000.003932	9.801549	-0.097010	4.817857
497.307601	8000.010930	9.806554	-0.096909	4.817861
497.315103	8000.075300	9.811559	-0.096910	4.817880
497.430148	8000.012675	9.816563	-0.096931	4.817861
497.612666	7999.968921	9.821568	-0.096965	4.817847
497.846370	8000.001751	9.826573	-0.097009	4.817856
497.743008	7999.959189	9.831578	-0.096990	4.817844
497.524007	8000.036132	9.836583	-0.096949	4.817868
497.068810	8000.021214	9.841587	-0.096864	4.817865
497.067991	8000.067555	9.846592	-0.096864	4.817879
497.110782	8000.094502	9.851597	-0.096872	4.817887
497.059230	8000.040037	9.856602	-0.096862	4.817871
497.089767	8000.110003	9.861607	-0.096868	4.817891
496.671257	8000.107196	9.866611	-0.096790	4.817892
497.085628	8000.094139	9.871616	-0.096867	4.817887
496.955574	8000.117568	9.876621	-0.096843	4.817894
497.436272	8000.031711	9.881626	-0.096932	4.817867
496.944083	8000.136365	9.886631	-0.096841	4.817900
497.067801	8000.095987	9.891635	-0.096864	4.817887
497.674828	8000.069875	9.896640	-0.096977	4.817877
498.282194	8000.036395	9.901645	-0.097090	4.817865
497.825559	8000.013025	9.906650	-0.097005	4.817860
498.039176	8000.096139	9.911655	-0.097045	4.817883
497.908029	8000.087946	9.916659	-0.097020	4.817881
498.185951	8000.017108	9.921664	-0.097072	4.817859
497.978226	8000.076303	9.926669	-0.097033	4.817878
497.919698	8000.023844	9.931674	-0.097022	4.817862
498.378902	8000.000893	9.936679	-0.097108	4.817854
498.072011	8000.009157	9.941683	-0.097051	4.817857
497.923271	8000.012303	9.946688	-0.097023	4.817859
498.057996	8000.075328	9.951693	-0.097048	4.817877
497.754799	8000.016219	9.956698	-0.096991	4.817861
497.709998	8000.113557	9.961703	-0.096983	4.817890
497.915611	8000.073294	9.966707	-0.097021	4.817877
498.117910	8000.066696	9.971712	-0.097059	4.817874
497.491271	8000.096739	9.976717	-0.096942	4.817886
497.587677	8000.074935	9.981722	-0.096960	4.817879
497.751787	8000.110987	9.986727	-0.096991	4.817889
497.318816	8000.107972	9.991731	-0.096910	4.817890
496.969076	8000.157767	9.996736	-0.096845	4.817906
497.272850	8000.126278	10.001741	-0.096902	4.817896
497.086610	8000.124675	10.006746	-0.096867	4.817896
497.172206	8000.122733	10.011751	-0.096883	4.817895
497.671994	8000.046631	10.016755	-0.096976	4.817870
497.800474	8000.037927	10.021760	-0.097000	4.817867
497.460061	8000.102604	10.026765	-0.096936	4.817888
497.287003	8000.122259	10.031770	-0.096904	4.817894
497.152469	8000.198300	10.036775	-0.096879	4.817917
497.349369	8000.147377	10.041779	-0.096916	4.817901
497.488169	8000.124071	10.046784	-0.096942	4.817894
497.757064	8000.102620	10.051789	-0.096992	4.817886
497.544036	8000.104848	10.056794	-0.096952	4.817888
497.629299	8000.108170	10.061799	-0.096968	4.817889
497.608303	8000.111030	10.066803	-0.096964	4.817890
497.424784	8000.110519	10.071808	-0.096930	4.817890
497.225404	8000.180368	10.076813	-0.096893	4.817912
497.176928	8000.115411	10.081818	-0.096884	4.817893
497.544054	8000.172267	10.086823	-0.096952	4.817908
497.544182	8000.142769	10.091827	-0.096952	4.817899
497.920801	8000.077553	10.096832	-0.097022	4.817878
498.248149	8000.076953	10.101837	-0.097083	4.817877
498.140740	8000.068045	10.106842	-0.097063	4.817875
498.301192	8000.086136	10.111847	-0.097093	4.817879
498.183502	8000.065493	10.116851	-0.097071	4.817874
498.475641	8000.049641	10.121856	-0.097125	4.817868
498.525748	8000.067212	10.126861	-0.097134	4.817873
498.257968	8000.053909	10.131866	-0.097085	4.817870
498.076465	8000.106103	10.136871	-0.097051	4.817886
498.160776	8000.082019	10.141875	-0.097067	4.817879
498.332764	8000.067615	10.146880	-0.097099	4.817874
498.464464	8000.096885	10.151885	-0.097123	4.817882
497.995713	8000.047002	10.156890	-0.097036	4.817869
498.201399	8000.105772	10.161895	-0.097074	4.817886
498.264633	8000.085602	10.166899	-0.097086	4.817879
498.340785	8000.071938	10.171904	-0.097100	4.817875
498.259289	8000.084471	10.176909	-0.097085	4.817879
498.427985	8000.082662	10.181914	-0.097116	4.817878
498.008082	8000.133562	10.186919	-0.097038	4.817895
498.535415	8000.047318	10.191923	-0.097136	4.817867
498.227678	8000.072426	10.196928	-0.097079	4.817876
498.299308	8000.093464	10.201933	-0.097092	4.817881
498.667122	8000.058676	10.206938	-0.097161	4.817870
498.565533	8000.063546	10.211943	-0.097142	4.817872
498.691187	7999.993697	10.216947	-0.097165	4.817850
498.629474	8000.012833	10.221952	-0.097153	4.817856
498.534197	8000.055721	10.226957	-0.097136	4.817869
498.058224	8000.093179	10.231962	-0.097047	4.817882
497.921988	8000.116520	10.236967	-0.097022	4.817890
498.082145	8000.054538	10.241971	-0.097052	4.817871
498.239861	8000.061000	10.246976	-0.097081	4.817872
498.170472	8000.087401	10.251981	-0.097068	4.817880
498.253705	8000.056981	10.256986	-0.097083	4.817871
498.367644	8000.100747	10.261991	-0.097105	4.817883
498.201799	8000.080470	10.266995	-0.097074	4.817878
498.302839	8000.052411	10.272000	-0.097093	4.817869
498.440563	8000.067017	10.277005	-0.097118	4.817873
498.253378	8000.095952	10.282010	-0.097083	4.817882
498.329382	8000.109678	10.287015	-0.097097	4.817886
498.154610	8000.125093	10.292019	-0.097065	4.817891
498.353277	8000.138462	10.297024	-0.097102	4.817895
498.339321	8000.165654	10.302029	-0.097099	4.817903
499.007068	8000.051915	10.307034	-0.097224	4.817866
498.633994	8000.106643	10.312039	-0.097154	4.817884
498.621091	8000.072744	10.317043	-0.097152	4.817874
498.454476	8000.123043	10.322048	-0.097121	4.817890
498.825586	8000.074606	10.327053	-0.097190	4.817874
498.188377	8000.100281	10.332058	-0.097071	4.817884
498.234514	8000.129384	10.337063	-0.097080	4.817892
498.311645	8000.135751	10.342067	-0.097094	4.817894
498.315204	8000.098927	10.347072	-0.097095	4.817883
498.279568	8000.107899	10.352077	-0.097088	4.817886
498.578397	8000.066859	10.357082	-0.097144	4.817872
498.322581	8000.123260	10.362087	-0.097096	4.817890
498.255029	8000.119135	10.367091	-0.097083	4.817889
498.060216	8000.126890	10.372096	-0.097047	4.817892
497.826855	8000.189933	10.377101	-0.097004	4.817912
497.922619	8000.127032	10.382106	-0.097021	4.817893
498.218031	8000.149155	10.387111	-0.097077	4.817898
498.431322	8000.145876	10.392115	-0.097116	4.817896
498.518717	8000.138693	10.397120	-0.097132	4.817894
498.338030	8000.182470	10.402125	-0.097099	4.817908
498.867174	8000.102574	10.407130	-0.097197	4.817882
498.797675	8000.100528	10.412135	-0.097184	4.817881
498.888398	8000.100768	10.417139	-0.097201	4.817881
498.753698	8000.149415	10.422144	-0.097176	4.817896
498.868407	8000.093105	10.427149	-0.097197	4.817879
498.581384	8000.098491	10.432154	-0.097144	4.817882
499.153334	8000.033956	10.437159	-0.097250	4.817860
499.434833	8000.064311	10.442163	-0.097303	4.817868
499.472228	8000.045879	10.447168	-0.097310	4.817862
499.103236	8000.072219	10.452173	-0.097241	4.817872
498.599750	8000.066088	10.457178	-0.097147	4.817872
498.387827	8000.142079	10.462183	-0.097108	4.817896
497.926130	8000.157616	10.467187	-0.097022	4.817902
498.308569	8000.120929	10.472192	-0.097093	4.817890
498.420114	8000.175196	10.477197	-0.097114	4.817905
498.524630	8000.081867	10.482202	-0.097133	4.817877
498.531332	8000.165192	10.487207	-0.097135	4.817902
498.671374	8000.131368	10.492211	-0.097161	4.817891
498.854698	8000.097109	10.497216	-0.097195	4.817880
498.953336	8000.111158	10.502221	-0.097213	4.817884
499.002364	8000.092892	10.507226	-0.097222	4.817878
499.473690	8000.064850	10.512231	-0.097310	4.817868
498.978354	8000.110458	10.517235	-0.097218	4.817884
498.807791	8000.091166	10.522240	-0.097186	4.817879
498.944689	8000.132100	10.527245	-0.097211	4.817890
498.833092	8000.122078	10.532250	-0.097191	4.817888
498.869342	8000.161576	10.537255	-0.097197	4.817899
498.883070	8000.123842	10.542259	-0.097200	4.817888
499.084350	8000.108803	10.547264	-0.097237	4.817883
498.751484	8000.143034	10.552269	-0.097175	4.817894
498.682673	8000.124140	10.557274	-0.097163	4.817889
498.871168	8000.139472	10.562279	-0.097198	4.817893
498.645565	8000.126769	10.567283	-0.097156	4.817890
498.873589	8000.120540	10.572288	-0.097198	4.817887
498.957560	8000.118576	10.577293	-0.097214	4.817886
498.911193	8000.094735	10.582298	-0.097205	4.817879
499.018595	8000.089946	10.587303	-0.097225	4.817877
498.912213	8000.116872	10.592307	-0.097205	4.817886
498.237690	8000.174674	10.597312	-0.097080	4.817906
498.738045	8000.116492	10.602317	-0.097173	4.817886
498.404790	8000.157039	10.607322	-0.097111	4.817900
498.520192	8000.187130	10.612327	-0.097132	4.817908
498.582579	8000.169055	10.617331	-0.097144	4.817903
499.031738	8000.127000	10.622336	-0.097227	4.817888
499.090957	8000.116255	10.627341	-0.097238	4.817885
499.179047	8000.090118	10.632346	-0.097255	4.817877
499.390175	8000.091023	10.637351	-0.097294	4.817876
499.508511	8000.061104	10.642355	-0.097316	4.817867
499.012788	8000.142527	10.647360	-0.097224	4.817893
499.144160	8000.130705	10.652365	-0.097248	4.817889
499.338476	8000.114513	10.657370	-0.097284	4.817883
498.940785	8000.166782	10.662375	-0.097210	4.817901
498.841331	8000.145344	10.667379	-0.097192	4.817895
498.651844	8000.173192	10.672384	-0.097156	4.817904
499.146132	8000.171816	10.677389	-0.097248	4.817901
498.972085	8000.099796	10.682394	-0.097216	4.817881
498.907140	8000.144172	10.687399	-0.097204	4.817894
498.904264	8000.149397	10.692403	-0.097203	4.817896
498.951876	8000.116362	10.697408	-0.097212	4.817886
498.976835	8000.148323	10.702413	-0.097217	4.817895
498.749745	8000.126118	10.707418	-0.097175	4.817889
498.964058	8000.130228	10.712423	-0.097214	4.817890
499.225146	8000.093918	10.717427	-0.097263	4.817878
499.124122	8000.116707	10.722432	-0.097244	4.817885
499.388243	8000.112047	10.727437	-0.097293	4.817882
499.403718	8000.083820	10.732442	-0.097296	4.817874
499.107419	8000.104876	10.737447	-0.097241	4.817881
499.029776	8000.154338	10.742451	-0.097227	4.817896
499.125519	8000.112507	10.747456	-0.097244	4.817884
499.047254	8000.159853	10.752461	-0.097230	4.817898
498.918762	8000.126411	10.757466	-0.097206	4.817889
499.238077	8000.145717	10.762471	-0.097265	4.817893
499.285940	8000.115846	10.767475	-0.097274	4.817884
499.087549	8000.113013	10.772480	-0.097237	4.817884
499.929509	8000.075512	10.777485	-0.097394	4.817869
499.643461	8000.041928	10.782490	-0.097341	4.817861
498.955379	8000.156427	10.787495	-0.097213	4.817897
499.324456	8000.090051	10.792499	-0.097281	4.817876
499.199807	8000.111449	10.797504	-0.097258	4.817883
499.538399	8000.117334	10.802509	-0.097321	4.817883
498.897722	8000.160868	10.807514	-0.097202	4.817899
499.075322	8000.174990	10.812519	-0.097235	4.817902
499.727179	8000.065240	10.817523	-0.097356	4.817867
499.735555	8000.029537	10.822528	-0.097358	4.817857
499.717516	8000.115671	10.827533	-0.097354	4.817882
499.813463	8000.060147	10.832538	-0.097372	4.817865
499.528389	8000.107702	10.837543	-0.097319	4.817881
499.596707	8000.131854	10.842547	-0.097332	4.817887
499.589256	8000.096979	10.847552	-0.097330	4.817877
499.630149	8000.112312	10.852557	-0.097338	4.817881
499.246815	8000.134232	10.857562	-0.097267	4.817890
499.069303	8000.199125	10.862567	-0.097234	4.817910
499.474722	8000.123786	10.867571	-0.097309	4.817886
499.302052	8000.107624	10.872576	-0.097277	4.817881
499.266059	8000.158734	10.877581	-0.097270	4.817897
499.837070	8000.093134	10.882586	-0.097377	4.817875
499.556025	8000.127049	10.887591	-0.097324	4.817886
499.580652	8000.118971	10.892595	-0.097329	4.817884
499.770608	8000.091128	10.897600	-0.097364	4.817875
499.864607	8000.128290	10.902605	-0.097382	4.817885
499.838508	8000.106845	10.907610	-0.097377	4.817879
499.940609	8000.119891	10.912615	-0.097396	4.817882
499.879606	8000.130608	10.917619	-0.097384	4.817886
499.797754	8000.050421	10.922624	-0.097369	4.817862
499.791230	8000.139880	10.927629	-0.097368	4.817889
499.746482	8000.102365	10.932634	-0.097360	4.817878
500.002334	8000.064927	10.937639	-0.097407	4.817866
499.470827	8000.085786	10.942643	-0.097308	4.817874
499.736888	8000.050600	10.947648	-0.097358	4.817863
499.233122	8000.124533	10.952653	-0.097264	4.817887
499.069912	8000.114828	10.957658	-0.097233	4.817885
499.317522	8000.126789	10.962663	-0.097280	4.817887
499.623335	8000.081635	10.967667	-0.097336	4.817872
499.539854	8000.077282	10.972672	-0.097321	4.817872
499.285320	8000.156880	10.977677	-0.097274	4.817896
499.206536	8000.143111	10.982682	-0.097259	4.817892
499.337905	8000.147092	10.987687	-0.097283	4.817893
499.523059	8000.128663	10.992691	-0.097318	4.817887
499.571722	8000.154642	10.997696	-0.097327	4.817894
499.640565	8000.133499	11.002701	-0.097340	4.817888
499.504075	8000.079924	11.007706	-0.097314	4.817872
499.116056	8000.182902	11.012711	-0.097242	4.817905
499.836746	8000.122599	11.017715	-0.097376	4.817884
499.547141	8000.132161	11.022720	-0.097322	4.817888
499.380727	8000.155070	11.027725	-0.097291	4.817895
499.280067	8000.118864	11.032730	-0.097272	4.817885
499.529289	8000.119260	11.037735	-0.097319	4.817884
499.543358	8000.088906	11.042739	-0.097321	4.817875
499.588882	8000.143287	11.047744	-0.097330	4.817891
499.584613	8000.112671	11.052749	-0.097329	4.817882
499.115547	8000.122832	11.057754	-0.097242	4.817887
499.307077	8000.154011	11.062759	-0.097277	4.817895
499.339639	8000.154475	11.067763	-0.097283	4.817895
499.332388	8000.152263	11.072768	-0.097282	4.817895
499.557265	8000.132293	11.077773	-0.097324	4.817888
499.458686	8000.100331	11.082778	-0.097305	4.817879
499.602198	8000.138200	11.087783	-0.097332	4.817889
499.712128	8000.099732	11.092787	-0.097353	4.817877
499.590543	8000.113799	11.097792	-0.097330	4.817882
499.861105	8000.125036	11.102797	-0.097380	4.817884
499.834469	8000.062493	11.107802	-0.097375	4.817866
499.163618	8000.119292	11.112807	-0.097250	4.817886
499.381661	8000.105546	11.117811	-0.097291	4.817881
499.485034	8000.114395	11.122816	-0.097310	4.817883
499.447599	8000.158109	11.127821	-0.097303	4.817896
499.857836	8000.098643	11.132826	-0.097380	4.817876
499.739545	8000.114864	11.137831	-0.097358	4.817882
499.503805	8000.124141	11.142835	-0.097314	4.817886
499.646478	8000.101944	11.147840	-0.097340	4.817878
499.591585	8000.133820	11.152845	-0.097330	4.817888
499.088452	8000.146655	11.157850	-0.097236	4.817894
499.463058	8000.102483	11.162855	-0.097306	4.817879
499.606287	8000.116116	11.167859	-0.097333	4.817883
499.551423	8000.124814	11.172864	-0.097323	4.817886
499.543804	8000.107847	11.177869	-0.097321	4.817881
499.294801	8000.119042	11.182874	-0.097275	4.817885
499.371695	8000.118031	11.187879	-0.097289	4.817884
499.382724	8000.132937	11.192883	-0.097291	4.817889
499.531922	8000.132958	11.197888	-0.097319	4.817888
500.186927	8000.111754	11.202893	-0.097441	4.817879
500.109010	8000.074819	11.207898	-0.097426	4.817868
499.806025	8000.134761	11.212903	-0.097370	4.817887
499.963427	8000.081167	11.217907	-0.097399	4.817871
499.890234	8000.071693	11.222912	-0.097385	4.817868
499.729525	8000.126290	11.227917	-0.097356	4.817885
499.292830	8000.109520	11.232922	-0.097274	4.817882
499.750810	8000.137128	11.237927	-0.097359	4.817888
499.703529	8000.119595	11.242931	-0.097351	4.817883
499.818092	8000.060121	11.247936	-0.097372	4.817865
500.055617	8000.108815	11.252941	-0.097416	4.817879
499.627568	8000.106918	11.257946	-0.097336	4.817880
499.224100	8000.132765	11.262951	-0.097261	4.817889
499.486281	8000.098577	11.267955	-0.097310	4.817878
499.278008	8000.149335	11.272960	-0.097271	4.817894
499.840541	8000.125757	11.277965	-0.097376	4.817885
499.771292	8000.082624	11.282970	-0.097363	4.817872
499.828341	8000.107670	11.287975	-0.097374	4.817879
499.784807	8000.097565	11.292979	-0.097366	4.817876
499.906545	8000.053998	11.297984	-0.097388	4.817863
500.041682	8000.104391	11.302989	-0.097413	4.817877
499.858454	8000.095452	11.307994	-0.097379	4.817876
500.041899	8000.101231	11.312999	-0.097413	4.817876
499.405569	8000.175378	11.318003	-0.097295	4.817901
499.574718	8000.164095	11.323008	-0.097326	4.817897
499.823167	8000.130766	11.328013	-0.097373	4.817886
499.840237	8000.096240	11.333018	-0.097376	4.817876
499.869537	8000.145122	11.338023	-0.097381	4.817890
500.374855	8000.105978	11.343027	-0.097475	4.817876
500.209382	8000.024596	11.348032	-0.097444	4.817853
499.958054	8000.101079	11.353037	-0.097398	4.817877
499.773525	8000.104765	11.358042	-0.097363	4.817879
499.689668	8000.118317	11.363047	-0.097348	4.817883
499.928138	8000.121720	11.368051	-0.097392	4.817883
499.479656	8000.134281	11.373056	-0.097309	4.817889
499.407668	8000.184877	11.378061	-0.097295	4.817904
499.341634	8000.166023	11.383066	-0.097283	4.817899
499.498041	8000.187219	11.388071	-0.097312	4.817904
499.472867	8000.171055	11.393075	-0.097307	4.817900
499.066876	8000.169473	11.398080	-0.097232	4.817901
499.525547	8000.179179	11.403085	-0.097317	4.817902
499.266416	8000.179694	11.408090	-0.097269	4.817903
499.368957	8000.171674	11.413095	-0.097288	4.817900
499.200965	8000.226168	11.418099	-0.097257	4.817917
499.574284	8000.130353	11.423104	-0.097326	4.817887
499.723920	8000.125113	11.428109	-0.097354	4.817885
499.640735	8000.111281	11.433114	-0.097338	4.817881
499.900900	8000.113940	11.438119	-0.097387	4.817881
499.557576	8000.112199	11.443123	-0.097323	4.817882
499.750716	8000.087562	11.448128	-0.097359	4.817874
499.662459	8000.130551	11.453133	-0.097342	4.817887
499.846022	8000.102617	11.458138	-0.097377	4.817878
500.189388	8000.076964	11.463143	-0.097440	4.817869
499.900280	8000.079157	11.468147	-0.097387	4.817871
500.059475	8000.022428	11.473152	-0.097416	4.817853
500.162760	8000.071313	11.478157	-0.097435	4.817867
500.163483	8000.051304	11.483162	-0.097436	4.817861
500.001577	8000.118528	11.488167	-0.097405	4.817882
500.347174	8000.128729	11.493171	-0.097470	4.817883
500.069670	8000.094212	11.498176	-0.097418	4.817874
500.185441	8000.108506	11.503181	-0.097440	4.817878
499.675378	8000.125456	11.508186	-0.097345	4.817885
499.669993	8000.173842	11.513191	-0.097344	4.817900
499.634849	8000.147000	11.518195	-0.097337	4.817892
499.576796	8000.168295	11.523200	-0.097326	4.817898
499.789952	8000.158694	11.528205	-0.097366	4.817895
499.525554	8000.137008	11.533210	-0.097317	4.817889
499.299763	8000.252837	11.538215	-0.097275	4.817925
500.084840	8000.150258	11.543219	-0.097421	4.817891
499.674804	8000.166528	11.548224	-0.097344	4.817897
499.854817	8000.164883	11.553229	-0.097378	4.817896
499.911728	8000.124604	11.558234	-0.097388	4.817884
499.890610	8000.147481	11.563239	-0.097385	4.817891
499.646331	8000.126081	11.568243	-0.097339	4.817886
500.015554	8000.122923	11.573248	-0.097408	4.817883
500.168035	8000.143010	11.578253	-0.097436	4.817888
500.475813	8000.030455	11.583258	-0.097493	4.817854
500.746664	8000.063822	11.588263	-0.097544	4.817862
500.316940	8000.091400	11.593267	-0.097464	4.817872
500.006753	8000.128059	11.598272	-0.097406	4.817885
500.221900	8000.133237	11.603277	-0.097446	4.817885
500.470562	8000.084107	11.608282	-0.097492	4.817870
500.570916	8000.057092	11.613287	-0.097511	4.817861
500.609473	8000.051320	11.618291	-0.097518	4.817859
500.940048	7999.997039	11.623296	-0.097580	4.817842
501.064055	8000.038845	11.628301	-0.097603	4.817854
500.828309	8000.019673	11.633306	-0.097559	4.817849
500.506701	8000.070920	11.638311	-0.097499	4.817866
500.502964	8000.052955	11.643315	-0.097498	4.817860
500.058436	8000.118250	11.648320	-0.097416	4.817881
499.851834	8000.185890	11.653325	-0.097377	4.817902
500.140706	8000.100458	11.658330	-0.097431	4.817876
500.267343	8000.124391	11.663335	-0.097454	4.817882
499.867620	8000.128165	11.668339	-0.097380	4.817885
499.860972	8000.133337	11.673344	-0.097379	4.817887
499.962822	8000.143218	11.678349	-0.097398	4.817889
500.336738	8000.086394	11.683354	-0.097467	4.817871
500.380688	8000.081753	11.688359	-0.097475	4.817869
500.189784	8000.125384	11.693363	-0.097440	4.817883
499.918783	8000.074103	11.698368	-0.097389	4.817869
500.405826	8000.091591	11.703373	-0.097480	4.817872
499.794404	8000.205076	11.708378	-0.097366	4.817908
499.833419	8000.172971	11.713383	-0.097373	4.817899
499.502303	8000.171403	11.718387	-0.097312	4.817900
499.453794	8000.145424	11.723392	-0.097303	4.817892
499.819292	8000.188569	11.728397	-0.097371	4.817903
500.114300	8000.071618	11.733402	-0.097426	4.817867
499.839259	8000.126691	11.738407	-0.097374	4.817885
500.028573	8000.132553	11.743411	-0.097410	4.817886
499.609926	8000.153969	11.748416	-0.097332	4.817894
499.259373	8000.196374	11.753421	-0.097267	4.817908
499.176742	8000.174122	11.758426	-0.097251	4.817902
499.638274	8000.144888	11.763431	-0.097337	4.817891
499.171532	8000.224617	11.768435	-0.097250	4.817917
499.903825	8000.127605	11.773440	-0.097386	4.817885
500.214127	8000.117284	11.778445	-0.097444	4.817881
500.283285	8000.096145	11.783450	-0.097457	4.817874
499.595534	8000.175879	11.788455	-0.097329	4.817901
500.756344	8000.103952	11.793459	-0.097545	4.817874
500.372497	8000.107951	11.798464	-0.097474	4.817877
500.353935	8000.134025	11.803469	-0.097470	4.817885
500.024864	8000.116682	11.808474	-0.097409	4.817881
499.829720	8000.159199	11.813479	-0.097373	4.817895
500.517453	8000.083677	11.818483	-0.097500	4.817869
500.553722	8000.057854	11.823488	-0.097507	4.817862
500.320997	8000.118799	11.828493	-0.097464	4.817881
500.017365	8000.123945	11.833498	-0.097407	4.817883
500.221582	8000.153199	11.838503	-0.097445	4.817891
500.363093	8000.134147	11.843507	-0.097472	4.817885
499.835629	8000.122400	11.848512	-0.097373	4.817884
500.276967	8000.159255	11.853517	-0.097456	4.817893
500.207702	8000.120335	11.858522	-0.097443	4.817881
500.417464	8000.122276	11.863527	-0.097482	4.817881
500.447978	8000.109014	11.868531	-0.097487	4.817877
500.160005	8000.131240	11.873536	-0.097434	4.817885
499.923810	8000.180546	11.878541	-0.097390	4.817901
500.505330	8000.106669	11.883546	-0.097498	4.817876
500.166656	8000.153457	11.888551	-0.097435	4.817891
500.254485	8000.142067	11.893555	-0.097451	4.817888
500.322599	8000.134610	11.898560	-0.097464	4.817885
500.174616	8000.160943	11.903565	-0.097436	4.817894
500.078369	8000.121638	11.908570	-0.097419	4.817882
500.097867	8000.156684	11.913575	-0.097422	4.817893
500.302893	8000.119574	11.918579	-0.097460	4.817881
500.198655	8000.132835	11.923584	-0.097441	4.817885
500.313207	8000.166077	11.928589	-0.097462	4.817895
500.624622	8000.122058	11.933594	-0.097520	4.817880
500.129492	8000.168720	11.938599	-0.097428	4.817896
500.300417	8000.143766	11.943603	-0.097460	4.817888
500.422653	8000.107581	11.948608	-0.097482	4.817877
500.459768	8000.154468	11.953613	-0.097489	4.817891
500.797770	8000.134008	11.958618	-0.097552	4.817883
500.621823	8000.140976	11.963623	-0.097520	4.817886
500.536756	8000.140814	11.968627	-0.097504	4.817886
500.223925	8000.139506	11.973632	-0.097445	4.817887
500.754719	8000.127067	11.978637	-0.097544	4.817881
500.305144	8000.137503	11.983642	-0.097461	4.817886
500.501096	8000.132925	11.988647	-0.097497	4.817884
500.762446	8000.111370	11.993651	-0.097546	4.817876
500.959751	8000.079418	11.998656	-0.097582	4.817866
500.746063	8000.120616	12.003661	-0.097543	4.817879
500.106173	8000.104102	12.008666	-0.097423	4.817877
500.583620	8000.108812	12.013671	-0.097512	4.817876
500.697124	8000.127289	12.018675	-0.097533	4.817881
500.194348	8000.097983	12.023680	-0.097440	4.817875
500.194839	8000.144347	12.028685	-0.097440	4.817889
499.965701	8000.153717	12.033690	-0.097397	4.817892
499.678730	8000.233905	12.038695	-0.097344	4.817917
500.424640	8000.168697	12.043699	-0.097483	4.817895
500.567903	8000.098044	12.048704	-0.097509	4.817873
500.401670	8000.173635	12.053709	-0.097478	4.817896
500.493168	8000.116992	12.058714	-0.097495	4.817879
500.032103	8000.176784	12.063719	-0.097409	4.817899
500.162180	8000.160729	12.068723	-0.097434	4.817894
500.111715	8000.139989	12.073728	-0.097424	4.817888
500.227096	8000.145850	12.078733	-0.097446	4.817889
499.861153	8000.154320	12.083738	-0.097378	4.817893
500.315550	8000.157647	12.088743	-0.097462	4.817892
500.336824	8000.134770	12.093747	-0.097466	4.817885
499.948184	8000.175578	12.098752	-0.097394	4.817899
500.304499	8000.162753	12.103757	-0.097460	4.817894
500.203526	8000.141292	12.108762	-0.097441	4.817888
500.257041	8000.143109	12.113767	-0.097451	4.817888
500.288711	8000.128810	12.118771	-0.097457	4.817884
499.820601	8000.165322	12.123776	-0.097370	4.817896
500.010910	8000.171199	12.128781	-0.097405	4.817897
499.800190	8000.142903	12.133786	-0.097366	4.817890
500.446774	8000.117366	12.138791	-0.097486	4.817880
500.494514	8000.107511	12.143795	-0.097495	4.817876
500.512473	8000.103551	12.148800	-0.097499	4.817875
500.699493	8000.120972	12.153805	-0.097533	4.817880
500.797279	8000.079169	12.158810	-0.097552	4.817867
500.604261	8000.067983	12.163815	-0.097516	4.817864
500.290756	8000.139364	12.168819	-0.097457	4.817887
500.915913	8000.068217	12.173824	-0.097574	4.817863
500.768384	8000.114575	12.178829	-0.097546	4.817877
500.214766	8000.135115	12.183834	-0.097443	4.817886
500.445950	8000.139468	12.188839	-0.097486	4.817886
500.874104	8000.125564	12.193843	-0.097566	4.817880
500.484438	8000.145284	12.198848	-0.097493	4.817888
500.479243	8000.169441	12.203853	-0.097492	4.817895
500.511837	8000.130923	12.208858	-0.097498	4.817883
500.363687	8000.129860	12.213863	-0.097471	4.817884
500.839400	8000.106098	12.218867	-0.097559	4.817875
500.638811	8000.087428	12.223872	-0.097522	4.817870
500.414807	8000.171676	12.228877	-0.097480	4.817896
500.202888	8000.186560	12.233882	-0.097441	4.817901
500.104111	8000.166184	12.238887	-0.097422	4.817896
500.080279	8000.185861	12.243891	-0.097418	4.817901
500.001416	8000.164715	12.248896	-0.097403	4.817896
500.199786	8000.172815	12.253901	-0.097440	4.817897
500.055548	8000.177075	12.258906	-0.097413	4.817899
500.424270	8000.107535	12.263911	-0.097482	4.817877
499.876498	8000.194535	12.268915	-0.097380	4.817905
499.999798	8000.123597	12.273920	-0.097403	4.817883
500.157205	8000.158504	12.278925	-0.097432	4.817893
500.429555	8000.152910	12.283930	-0.097483	4.817890
500.704794	8000.085195	12.288935	-0.097534	4.817869
500.515664	8000.116208	12.293939	-0.097499	4.817879
500.343362	8000.144301	12.298944	-0.097467	4.817888
500.672870	8000.140577	12.303949	-0.097528	4.817886
500.954091	8000.085590	12.308954	-0.097580	4.817868
501.009623	8000.080061	12.313959	-0.097591	4.817866
500.845196	8000.104051	12.318963	-0.097560	4.817874
500.892987	8000.064696	12.323968	-0.097569	4.817862
500.365293	8000.163572	12.328973	-0.097471	4.817894
501.140169	8000.086135	12.333978	-0.097615	4.817867
500.601508	8000.144818	12.338983	-0.097515	4.817887
501.008204	8000.078980	12.343987	-0.097590	4.817866
500.861905	8000.028424	12.348992	-0.097563	4.817852
500.421212	8000.135918	12.353997	-0.097481	4.817885
500.409631	8000.128376	12.359002	-0.097479	4.817883
500.457633	8000.118525	12.364007	-0.097488	4.817880
501.126489	8000.092254	12.369011	-0.097612	4.817869
501.112742	8000.029894	12.374016	-0.097610	4.817851
500.820033	8000.087875	12.379021	-0.097555	4.817869
501.285551	8000.057646	12.384026	-0.097642	4.817858
501.063381	8000.081866	12.389031	-0.097601	4.817867
501.015560	8000.099093	12.394035	-0.097592	4.817872
501.155060	8000.070530	12.399040	-0.097618	4.817863
500.801978	8000.117112	12.404045	-0.097552	4.817878
500.688218	8000.111272	12.409050	-0.097531	4.817877
500.366306	8000.144603	12.414055	-0.097471	4.817888
500.843988	8000.141942	12.419059	-0.097560	4.817885
500.697148	8000.140897	12.424064	-0.097532	4.817886
500.934015	8000.108456	12.429069	-0.097576	4.817875
501.220222	8000.020880	12.434074	-0.097630	4.817848
500.728689	8000.132915	12.439079	-0.097538	4.817883
501.248145	8000.081332	12.444083	-0.097635	4.817866
501.708925	7999.982552	12.449088	-0.097720	4.817834
501.587651	8000.057732	12.454093	-0.097698	4.817857
501.525490	8000.039985	12.459098	-0.097686	4.817852
500.990121	8000.071320	12.464103	-0.097587	4.817864
501.011623	8000.132735	12.469107	-0.097591	4.817882
501.159971	8000.121156	12.474112	-0.097618	4.817878
501.003637	8000.123137	12.479117	-0.097589	4.817879
501.250304	8000.060282	12.484122	-0.097635	4.817859
501.288346	8000.021840	12.489127	-0.097642	4.817848
501.216485	8000.080869	12.494131	-0.097629	4.817866
500.987217	8000.037556	12.499136	-0.097586	4.817854
501.260127	8000.081490	12.504141	-0.097637	4.817866
500.992510	8000.036576	12.509146	-0.097587	4.817853
501.257126	7999.995049	12.514151	-0.097636	4.817840
501.144066	8000.073507	12.519155	-0.097615	4.817864
501.172674	8000.050735	12.524160	-0.097620	4.817857
500.624838	8000.126144	12.529165	-0.097518	4.817881
501.041889	8000.050972	12.534170	-0.097596	4.817857
500.686508	8000.095415	12.539175	-0.097530	4.817872
500.711266	8000.140018	12.544179	-0.097535	4.817885
500.454693	8000.113174	12.549184	-0.097487	4.817878
501.101481	8000.044444	12.554189	-0.097607	4.817855
501.022524	8000.094941	12.559194	-0.097592	4.817871
501.699138	7999.932867	12.564199	-0.097718	4.817820
501.104614	8000.053968	12.569203	-0.097608	4.817858
501.045119	8000.053117	12.574208	-0.097597	4.817858
501.135783	8000.084965	12.579213	-0.097613	4.817867
500.685532	8000.123838	12.584218	-0.097530	4.817881
500.814753	8000.127790	12.589223	-0.097554	4.817881
500.833390	8000.139644	12.594227	-0.097557	4.817885
500.554989	8000.136721	12.599232	-0.097505	4.817885
500.794609	8000.155946	12.604237	-0.097550	4.817890
500.664908	8000.123538	12.609242	-0.097526	4.817881
501.023054	8000.126545	12.614247	-0.097592	4.817880
501.089447	8000.131707	12.619251	-0.097605	4.817881
500.675453	8000.171097	12.624256	-0.097528	4.817895
500.550641	8000.164046	12.629261	-0.097504	4.817893
500.242821	8000.153327	12.634266	-0.097447	4.817891
501.003239	8000.074630	12.639271	-0.097589	4.817865
501.152602	8000.072548	12.644275	-0.097616	4.817863
500.095271	8000.144895	12.649280	-0.097420	4.817889
500.207881	8000.179164	12.654285	-0.097441	4.817899
500.569042	8000.159034	12.659290	-0.097508	4.817891
500.989862	8000.099720	12.664295	-0.097586	4.817872
500.903974	8000.139583	12.669299	-0.097570	4.817884
500.939520	8000.095838	12.674304	-0.097577	4.817871
501.512862	8000.022898	12.679309	-0.097683	4.817847
501.420772	8000.038440	12.684314	-0.097666	4.817852
501.542185	8000.027529	12.689319	-0.097689	4.817848
501.859094	8000.045753	12.694323	-0.097748	4.817852
501.139208	8000.070237	12.699328	-0.097614	4.817863
501.319219	8000.099148	12.704333	-0.097647	4.817871
501.112010	8000.100401	12.709338	-0.097609	4.817872
501.099538	8000.078096	12.714343	-0.097606	4.817865
501.009542	8000.138972	12.719347	-0.097590	4.817884
501.272458	8000.088993	12.724352	-0.097638	4.817868
501.210306	8000.143945	12.729357	-0.097627	4.817884
501.143031	8000.090302	12.734362	-0.097614	4.817869
501.396228	8000.018058	12.739367	-0.097661	4.817846
501.243461	8000.093842	12.744371	-0.097633	4.817869
501.402316	8000.059234	12.749376	-0.097663	4.817858
501.059688	8000.128091	12.754381	-0.097599	4.817880
501.626317	8000.071914	12.759386	-0.097704	4.817861
501.437210	8000.051300	12.764391	-0.097669	4.817856
501.468097	8000.095992	12.769395	-0.097675	4.817869
501.637695	8000.030982	12.774400	-0.097706	4.817849
501.495970	8000.065833	12.779405	-0.097680	4.817860
501.190734	8000.095187	12.784410	-0.097623	4.817870
501.229166	8000.065180	12.789415	-0.097630	4.817861
501.105895	8000.111885	12.794419	-0.097607	4.817875
500.760295	8000.116430	12.799424	-0.097543	4.817878
501.588711	8000.056616	12.804429	-0.097697	4.817857
501.675538	8000.062070	12.809434	-0.097713	4.817858
501.127041	8000.101646	12.814439	-0.097611	4.817872
501.558243	8000.040374	12.819443	-0.097691	4.817852
501.411715	8000.055137	12.824448	-0.097664	4.817857
501.482105	8000.056142	12.829453	-0.097677	4.817857
500.784690	8000.112556	12.834458	-0.097547	4.817877
500.907515	8000.117470	12.839463	-0.097570	4.817878
501.540278	8000.073827	12.844467	-0.097688	4.817862
501.354452	8000.043777	12.849472	-0.097653	4.817854
501.161269	8000.094751	12.854477	-0.097617	4.817870
501.279304	8000.091168	12.859482	-0.097639	4.817868
501.470469	8000.002233	12.864487	-0.097675	4.817841
501.562291	8000.062546	12.869491	-0.097692	4.817859
501.219195	8000.055537	12.874496	-0.097628	4.817858
501.562108	8000.054113	12.879501	-0.097692	4.817856
501.568901	8000.096353	12.884506	-0.097693	4.817869
501.350929	8000.074273	12.889511	-0.097653	4.817863
501.260673	8000.119342	12.894515	-0.097636	4.817877
501.787133	8000.013071	12.899520	-0.097734	4.817843
501.193272	8000.094143	12.904525	-0.097623	4.817870
501.723887	8000.088026	12.909530	-0.097722	4.817866
501.597141	8000.019836	12.914535	-0.097698	4.817846
501.489457	8000.059388	12.919539	-0.097678	4.817858
501.611223	7999.992641	12.924544	-0.097701	4.817838
501.321514	8000.077005	12.929549	-0.097647	4.817864
501.158703	8000.103126	12.934554	-0.097617	4.817872
501.217899	8000.098702	12.939559	-0.097628	4.817871
501.016380	8000.121109	12.944563	-0.097590	4.817878
501.136686	8000.097540	12.949568	-0.097613	4.817871
501.605945	8000.046293	12.954573	-0.097700	4.817854
501.461663	8000.077947	12.959578	-0.097673	4.817864
501.530313	8000.082087	12.964583	-0.097686	4.817865
501.311823	8000.117948	12.969587	-0.097645	4.817876
501.375496	8000.061962	12.974592	-0.097657	4.817859
501.127750	8000.133228	12.979597	-0.097611	4.817881
500.779630	8000.169345	12.984602	-0.097546	4.817894
500.731965	8000.171824	12.989607	-0.097537	4.817895
501.127993	8000.144818	12.994611	-0.097611	4.817885
500.902329	8000.104717	12.999616	-0.097569	4.817874
500.865099	8000.134739	13.004621	-0.097562	4.817883
501.030060	8000.122344	13.009626	-0.097593	4.817879
500.870696	8000.151674	13.014631	-0.097563	4.817888
501.212372	8000.159715	13.019635	-0.097626	4.817889
501.067090	8000.102851	13.024640	-0.097599	4.817873
501.240293	8000.115860	13.029645	-0.097632	4.817876
501.511501	8000.107090	13.034650	-0.097682	4.817872
501.237707	8000.105285	13.039655	-0.097631	4.817873
501.007773	8000.147304	13.044659	-0.097588	4.817886
500.874251	8000.113788	13.049664	-0.097563	4.817877
500.674650	8000.157294	13.054669	-0.097526	4.817891
500.879548	8000.111754	13.059674	-0.097564	4.817876
501.082396	8000.097792	13.064679	-0.097602	4.817871
501.413086	8000.145713	13.069683	-0.097664	4.817884
500.841895	8000.112266	13.074688	-0.097557	4.817876
500.996632	8000.116583	13.079693	-0.097586	4.817877
501.262292	8000.076125	13.084698	-0.097636	4.817864
501.113864	8000.109826	13.089703	-0.097608	4.817875
501.614540	8000.109602	13.094707	-0.097701	4.817872
501.800684	8000.062741	13.099712	-0.097736	4.817858
501.694124	8000.050681	13.104717	-0.097716	4.817855
501.363209	8000.096526	13.109722	-0.097654	4.817870
501.284497	8000.106990	13.114727	-0.097640	4.817873
501.665606	8000.106112	13.119731	-0.097711	4.817871
501.460734	8000.068414	13.124736	-0.097672	4.817861
500.991539	8000.175501	13.129741	-0.097585	4.817895
501.237473	8000.142137	13.134746	-0.097631	4.817884
501.190323	8000.102478	13.139751	-0.097622	4.817872
501.406513	8000.079225	13.144755	-0.097662	4.817864
501.608452	8000.055769	13.149760	-0.097700	4.817857
501.281873	8000.090086	13.154765	-0.097639	4.817868
501.402806	8000.111831	13.159770	-0.097662	4.817874
501.459255	8000.113690	13.164775	-0.097672	4.817874
501.425664	8000.152193	13.169779	-0.097666	4.817886
501.113389	8000.126658	13.174784	-0.097608	4.817880
500.843457	8000.189179	13.179789	-0.097557	4.817899
500.916366	8000.203916	13.184794	-0.097571	4.817903
500.748223	8000.166744	13.189799	-0.097540	4.817893
500.931971	8000.160939	13.194803	-0.097574	4.817891
500.944230	8000.168488	13.199808	-0.097576	4.817893
500.858693	8000.197820	13.204813	-0.097560	4.817902
500.902258	8000.213191	13.209818	-0.097568	4.817906
500.956285	8000.173925	13.214823	-0.097578	4.817894
500.594952	8000.257265	13.219827	-0.097511	4.817921
500.577336	8000.192743	13.224832	-0.097508	4.817901
500.768483	8000.198633	13.229837	-0.097543	4.817902
500.808661	8000.208688	13.234842	-0.097551	4.817905
500.405217	8000.182906	13.239847	-0.097476	4.817899
500.392942	8000.209070	13.244851	-0.097473	4.817907
500.304255	8000.195159	13.249856	-0.097457	4.817903
500.428523	8000.222219	13.254861	-0.097480	4.817911
500.694556	8000.164908	13.259866	-0.097529	4.817893
500.760578	8000.141618	13.264871	-0.097542	4.817886
500.673002	8000.184617	13.269875	-0.097525	4.817899
501.044071	8000.133021	13.274880	-0.097594	4.817882
500.398147	8000.238637	13.279885	-0.097474	4.817916
501.033769	8000.201357	13.284890	-0.097592	4.817902
501.094039	8000.129517	13.289895	-0.097604	4.817881
500.905282	8000.158428	13.294899	-0.097569	4.817890
500.684803	8000.148956	13.299904	-0.097527	4.817888
500.859582	8000.175685	13.304909	-0.097560	4.817895
500.751773	8000.191001	13.309914	-0.097540	4.817900
500.946879	8000.173768	13.314919	-0.097576	4.817894
501.117979	8000.203606	13.319923	-0.097608	4.817902
501.194538	8000.163607	13.324928	-0.097622	4.817890
501.139306	8000.172300	13.329933	-0.097612	4.817893
501.130676	8000.190087	13.334938	-0.097610	4.817898
500.906170	8000.193200	13.339943	-0.097569	4.817900
500.850370	8000.199777	13.344947	-0.097558	4.817902
501.109975	8000.092855	13.349952	-0.097606	4.817870
501.493584	8000.096227	13.354957	-0.097678	4.817869
501.665641	8000.107113	13.359962	-0.097710	4.817872
501.217290	8000.127047	13.364967	-0.097626	4.817879
501.287700	8000.152285	13.369971	-0.097640	4.817886
500.921979	8000.112290	13.374976	-0.097571	4.817876
500.468651	8000.192210	13.379981	-0.097487	4.817902
501.026347	8000.143280	13.384986	-0.097591	4.817885
500.807160	8000.168595	13.389991	-0.097550	4.817893
500.835303	8000.189015	13.394995	-0.097555	4.817899
500.911387	8000.150063	13.400000	-0.097569	4.817887
501.117363	8000.170916	13.405005	-0.097608	4.817893
501.063282	8000.150124	13.410010	-0.097598	4.817887
500.582260	8000.178021	13.415015	-0.097508	4.817897
501.616837	8000.079008	13.420019	-0.097701	4.817863
501.812594	8000.070214	13.425024	-0.097737	4.817860
501.429471	8000.106884	13.430029	-0.097666	4.817872
500.891050	8000.171891	13.435034	-0.097565	4.817894
500.963598	8000.140264	13.440039	-0.097579	4.817884
501.089841	8000.171568	13.445043	-0.097602	4.817893
501.605920	8000.082007	13.450048	-0.097698	4.817864
501.399070	8000.145428	13.455053	-0.097660	4.817884
501.629466	8000.105521	13.460058	-0.097703	4.817871
501.216228	8000.153350	13.465063	-0.097626	4.817887
501.480207	8000.159228	13.470067	-0.097675	4.817888
501.504366	8000.090033	13.475072	-0.097680	4.817867
501.330880	8000.142341	13.480077	-0.097647	4.817883
501.624504	8000.106498	13.485082	-0.097702	4.817872
501.691377	8000.049503	13.490087	-0.097714	4.817854
501.655871	8000.125909	13.495091	-0.097708	4.817877
501.864656	8000.047762	13.500096	-0.097746	4.817853
502.113170	8000.040776	13.505101	-0.097793	4.817850
502.024325	8000.072167	13.510106	-0.097776	4.817860
501.794724	8000.034116	13.515111	-0.097733	4.817849
501.514812	8000.118620	13.520115	-0.097681	4.817876
501.099964	8000.147461	13.525120	-0.097604	4.817886
501.687367	8000.084206	13.530125	-0.097713	4.817865
502.107442	8000.088100	13.535130	-0.097792	4.817864
501.699062	8000.065406	13.540135	-0.097716	4.817859
501.738979	8000.090209	13.545139	-0.097723	4.817866
502.034609	8000.064930	13.550144	-0.097778	4.817857
502.121751	8000.010332	13.555149	-0.097794	4.817841
502.152249	8000.046590	13.560154	-0.097800	4.817852
501.851101	8000.030696	13.565159	-0.097744	4.817848
502.060668	8000.103229	13.570163	-0.097783	4.817869
502.048295	8000.052477	13.575168	-0.097780	4.817854
502.016997	8000.064672	13.580173	-0.097775	4.817857
501.677333	8000.079836	13.585178	-0.097711	4.817863
500.766543	8000.125827	13.590183	-0.097542	4.817881
501.147123	8000.171299	13.595187	-0.097613	4.817893
501.585918	8000.111189	13.600192	-0.097694	4.817873
501.796440	8000.120518	13.605197	-0.097734	4.817875
502.130729	8000.083148	13.610202	-0.097796	4.817862
501.545986	8000.104294	13.615207	-0.097687	4.817871
501.841869	8000.111681	13.620211	-0.097742	4.817872
501.676142	8000.117741	13.625216	-0.097711	4.817875
501.975275	8000.094620	13.630221	-0.097767	4.817867
501.797348	8000.098398	13.635226	-0.097734	4.817868
501.662659	8000.083829	13.640231	-0.097709	4.817865
501.755432	8000.142049	13.645235	-0.097726	4.817881
501.187374	8000.126557	13.650240	-0.097620	4.817879
501.590113	8000.098594	13.655245	-0.097695	4.817869
501.701178	8000.140217	13.660250	-0.097716	4.817881
501.324436	8000.120083	13.665255	-0.097645	4.817877
501.269543	8000.166710	13.670259	-0.097635	4.817891
501.548914	8000.161218	13.675264	-0.097687	4.817888
501.456100	8000.158837	13.680269	-0.097670	4.817888
501.298756	8000.150266	13.685274	-0.097641	4.817886
501.537426	8000.126281	13.690279	-0.097685	4.817878
501.931868	8000.178276	13.695283	-0.097759	4.817891
501.527770	8000.159856	13.700288	-0.097683	4.817888
501.702231	8000.127579	13.705293	-0.097716	4.817877
501.428019	8000.200574	13.710298	-0.097665	4.817900
500.658083	8000.198002	13.715303	-0.097521	4.817903
500.698435	8000.233347	13.720307	-0.097529	4.817913
501.088447	8000.158843	13.725312	-0.097601	4.817889
501.066990	8000.158535	13.730317	-0.097597	4.817889
501.243611	8000.123127	13.735322	-0.097630	4.817878
501.340965	8000.129785	13.740327	-0.097648	4.817880
501.348613	8000.197324	13.745331	-0.097650	4.817900
501.111769	8000.132830	13.750336	-0.097606	4.817881
501.435860	8000.164853	13.755341	-0.097666	4.817890
501.645711	8000.156260	13.760346	-0.097705	4.817886
501.396551	8000.182201	13.765351	-0.097659	4.817895
501.546823	8000.174864	13.770355	-0.097687	4.817892
501.392527	8000.148425	13.775360	-0.097658	4.817885
500.997298	8000.200726	13.780365	-0.097584	4.817902
501.237739	8000.165176	13.785370	-0.097629	4.817891
501.165074	8000.154655	13.790375	-0.097615	4.817888
501.315010	8000.183136	13.795379	-0.097643	4.817896
501.241185	8000.099898	13.800384	-0.097630	4.817871
501.413776	8000.138186	13.805389	-0.097662	4.817882
502.222990	8000.100227	13.810394	-0.097812	4.817867
501.817640	8000.050182	13.815399	-0.097737	4.817854
501.630955	8000.115999	13.820403	-0.097702	4.817874
502.181524	8000.097524	13.825408	-0.097805	4.817867
501.863044	8000.153029	13.830413	-0.097745	4.817884
502.121980	8000.117744	13.835418	-0.097793	4.817873
501.940609	8000.117258	13.840423	-0.097760	4.817873
502.471506	8000.060572	13.845427	-0.097859	4.817854
501.696037	8000.082152	13.850432	-0.097714	4.817864
502.060442	8000.063125	13.855437	-0.097782	4.817857
501.964486	8000.090200	13.860442	-0.097764	4.817865
502.115194	8000.048100	13.865447	-0.097792	4.817852
501.864610	8000.106683	13.870451	-0.097745	4.817871
501.858000	8000.101319	13.875456	-0.097744	4.817869
501.804813	8000.139542	13.880461	-0.097734	4.817881
501.776069	8000.125433	13.885466	-0.097729	4.817876
501.579265	8000.133156	13.890471	-0.097692	4.817880
501.589650	8000.152269	13.895475	-0.097694	4.817885
501.780936	8000.103373	13.900480	-0.097730	4.817870
501.908958	8000.075700	13.905485	-0.097754	4.817861
501.835665	8000.154727	13.910490	-0.097740	4.817885
501.885608	8000.024790	13.915495	-0.097749	4.817846
501.795682	8000.080400	13.920499	-0.097732	4.817863
501.831286	8000.065103	13.925504	-0.097739	4.817858
501.959242	8000.071145	13.930509	-0.097763	4.817860
501.717145	8000.115097	13.935514	-0.097718	4.817874
501.751886	8000.061858	13.940519	-0.097724	4.817858
501.680184	8000.150390	13.945523	-0.097711	4.817884
501.494926	8000.107705	13.950528	-0.097676	4.817872
501.557440	8000.143366	13.955533	-0.097688	4.817883
502.096322	8000.140529	13.960538	-0.097788	4.817880
501.821215	8000.139758	13.965543	-0.097737	4.817881
500.997364	8000.227026	13.970547	-0.097584	4.817910
500.811221	8000.212776	13.975552	-0.097549	4.817906
501.322180	8000.193734	13.980557	-0.097644	4.817899
500.780108	8000.223919	13.985562	-0.097543	4.817910
500.710412	8000.173403	13.990567	-0.097530	4.817895
501.194693	8000.186641	13.995571	-0.097620	4.817897
501.323696	8000.163196	14.000576	-0.097644	4.817890
501.255990	8000.158013	14.005581	-0.097632	4.817888
501.042549	8000.203429	14.010586	-0.097592	4.817903
501.852941	8000.143361	14.015591	-0.097743	4.817881
501.713222	8000.174026	14.020595	-0.097717	4.817891
501.924844	8000.123314	14.025600	-0.097756	4.817875
502.164796	8000.047719	14.030605	-0.097801	4.817852
502.041280	8000.044899	14.035610	-0.097778	4.817852
501.796625	8000.056153	14.040615	-0.097732	4.817856
502.125086	8000.141975	14.045619	-0.097793	4.817880
502.443434	7999.988479	14.050624	-0.097853	4.817833
502.124559	7999.992350	14.055629	-0.097793	4.817836
502.027503	8000.094218	14.060634	-0.097775	4.817866
501.841059	8000.121054	14.065639	-0.097741	4.817875
501.891231	8000.164968	14.070643	-0.097750	4.817888
501.895492	8000.092328	14.075648	-0.097751	4.817866
501.963696	8000.089087	14.080653	-0.097763	4.817865
501.548082	8000.127399	14.085658	-0.097686	4.817878
501.817515	8000.101747	14.090663	-0.097736	4.817869
502.099103	8000.121574	14.095667	-0.097788	4.817874
501.883744	8000.131139	14.100672	-0.097748	4.817878
502.045741	8000.067074	14.105677	-0.097778	4.817858
502.224402	8000.047500	14.110682	-0.097812	4.817852
501.768133	8000.069427	14.115687	-0.097727	4.817860
501.896844	8000.129214	14.120691	-0.097751	4.817877
502.046466	8000.082884	14.125696	-0.097779	4.817863
501.885510	8000.073208	14.130701	-0.097749	4.817861
502.158704	8000.096076	14.135706	-0.097799	4.817866
501.898922	8000.102899	14.140711	-0.097751	4.817869
501.772172	8000.170626	14.145715	-0.097727	4.817890
501.700739	8000.107440	14.150720	-0.097714	4.817872
502.273730	8000.045034	14.155725	-0.097821	4.817851
502.069187	8000.123239	14.160730	-0.097783	4.817875
501.833786	8000.110392	14.165735	-0.097739	4.817872
502.293258	8000.115903	14.170739	-0.097824	4.817872
501.998191	8000.099041	14.175744	-0.097769	4.817868
502.061394	8000.072549	14.180749	-0.097781	4.817860
502.246189	8000.112066	14.185754	-0.097816	4.817871
501.934056	8000.075996	14.190759	-0.097757	4.817861
502.119314	8000.117626	14.195763	-0.097792	4.817873
501.373018	8000.142784	14.200768	-0.097653	4.817883
501.703610	8000.128542	14.205773	-0.097715	4.817878
501.973079	8000.137659	14.210778	-0.097765	4.817879
501.868863	8000.069790	14.215783	-0.097745	4.817860
502.417058	8000.040746	14.220787	-0.097847	4.817849
501.970415	8000.081775	14.225792	-0.097764	4.817863
501.909449	8000.142014	14.230797	-0.097753	4.817881
501.779976	8000.164396	14.235802	-0.097729	4.817888
501.826512	7999.315857	14.240807	-0.097737	4.817636

502.166335	7996.050717	14.245811	-0.097798	4.816667
501.870052	7990.587855	14.250816	-0.097739	4.815049
502.048061	7984.003002	14.255821	-0.097768	4.813096
501.548034	7976.810695	14.260826	-0.097670	4.810964
501.549020	7969.125869	14.265831	-0.097665	4.808683
501.539723	7961.384647	14.270835	-0.097659	4.806384
501.292466	7953.411831	14.275840	-0.097607	4.804017
501.547848	7945.544067	14.280845	-0.097650	4.801677
501.885359	7937.535213	14.285850	-0.097707	4.799294
501.489178	7929.580783	14.290855	-0.097628	4.796929
501.614536	7921.541480	14.295859	-0.097646	4.794535
501.616515	7913.617831	14.300864	-0.097642	4.792175
501.518727	7905.530350	14.305869	-0.097618	4.789766
501.644984	7897.578402	14.310874	-0.097636	4.787395
501.377580	7889.523236	14.315879	-0.097581	4.784993
501.116888	7881.631277	14.320883	-0.097528	4.782638
500.828452	7873.582015	14.325888	-0.097469	4.780236
500.991234	7865.524130	14.330893	-0.097494	4.777828
500.967915	7857.552826	14.335898	-0.097484	4.775446
501.174377	7849.500284	14.340903	-0.097517	4.773037
501.418624	7841.490731	14.345907	-0.097558	4.770640
500.968597	7833.576023	14.350912	-0.097469	4.768273
500.673469	7825.537750	14.355917	-0.097409	4.765866
500.924290	7817.580915	14.360922	-0.097450	4.763481
500.954726	7809.550886	14.365927	-0.097450	4.761074
501.053679	7801.525564	14.370931	-0.097464	4.758666
501.154003	7793.498046	14.375936	-0.097477	4.756257
500.768133	7785.442083	14.380941	-0.097400	4.753840
500.592487	7777.578230	14.385946	-0.097362	4.751478
500.027421	7769.477162	14.390951	-0.097252	4.749044
499.920149	7761.554586	14.395955	-0.097226	4.746662
500.498995	7753.426980	14.400960	-0.097329	4.744216
500.457516	7745.494302	14.405965	-0.097316	4.741828
500.252944	7737.481443	14.410970	-0.097273	4.739415
500.071345	7729.537151	14.415975	-0.097234	4.737022
500.414158	7721.495295	14.420979	-0.097292	4.734597
500.464913	7713.423216	14.425984	-0.097296	4.732162
500.333058	7705.398452	14.430989	-0.097267	4.729740
500.437973	7697.466333	14.435994	-0.097281	4.727345
500.140936	7689.404274	14.440999	-0.097220	4.724910
500.432069	7681.472203	14.446003	-0.097269	4.722512
500.934573	7673.419481	14.451008	-0.097358	4.720076
500.402878	7665.439661	14.456013	-0.097253	4.717663
500.296227	7657.489360	14.461018	-0.097228	4.715257
500.375479	7649.479317	14.466023	-0.097238	4.712830
500.394399	7641.460679	14.471027	-0.097236	4.710401
500.647146	7633.462884	14.476032	-0.097278	4.707975
500.584435	7625.398540	14.481037	-0.097261	4.705529
500.694502	7617.491495	14.486042	-0.097276	4.703129
499.791102	7609.512653	14.491047	-0.097103	4.700708
499.914053	7601.517330	14.496051	-0.097121	4.698279
500.392188	7593.466064	14.501056	-0.097204	4.695831
499.925036	7585.504114	14.506061	-0.097112	4.693410
500.120589	7577.484509	14.511066	-0.097143	4.690970
499.988733	7569.429821	14.516071	-0.097114	4.688518
499.614957	7561.541451	14.521075	-0.097039	4.686115
499.660376	7553.451845	14.526080	-0.097042	4.683650
499.839171	7545.444717	14.531085	-0.097070	4.681208
499.024818	7537.563484	14.536090	-0.096913	4.678804
498.627919	7529.560003	14.541095	-0.096834	4.676362
498.938045	7521.425805	14.546099	-0.096887	4.673877
498.975321	7513.447342	14.551104	-0.096888	4.671439
498.890466	7505.362501	14.556109	-0.096867	4.668968
498.941232	7497.422056	14.561114	-0.096872	4.666539
498.375914	7489.408084	14.566119	-0.096761	4.664086
498.605975	7481.484501	14.571123	-0.096799	4.661660
498.240993	7473.433671	14.576128	-0.096725	4.659194
498.401404	7465.469395	14.581133	-0.096750	4.656752
498.395019	7457.405255	14.586138	-0.096744	4.654279
498.648536	7449.411764	14.591143	-0.096786	4.651826
498.345997	7441.409800	14.596147	-0.096724	4.649369
497.935937	7433.453792	14.601152	-0.096643	4.646925
498.251922	7425.367315	14.606157	-0.096696	4.644440
498.061641	7417.508277	14.611162	-0.096656	4.642023
498.216771	7409.346019	14.616167	-0.096679	4.639512
498.212141	7401.409197	14.621171	-0.096673	4.637069
498.542543	7393.335563	14.626176	-0.096729	4.634582
498.420733	7385.389993	14.631181	-0.096701	4.632133
498.642636	7377.342106	14.636186	-0.096737	4.629652
498.797683	7369.368335	14.641191	-0.096761	4.627192
498.401651	7361.386277	14.646195	-0.096682	4.624728
498.234971	7353.460865	14.651200	-0.096646	4.622281
498.376911	7345.369530	14.656205	-0.096667	4.619780
497.982160	7337.500552	14.661210	-0.096588	4.617347
497.752680	7329.343945	14.666215	-0.096540	4.614824
497.653025	7321.430620	14.671219	-0.096517	4.612375
497.293054	7313.415325	14.676224	-0.096444	4.609893
497.309467	7305.394459	14.681229	-0.096442	4.607408
497.564060	7297.348063	14.686234	-0.096484	4.604913
497.854273	7289.289730	14.691239	-0.096533	4.602414
497.694727	7281.361804	14.696243	-0.096498	4.599954
497.395695	7273.450720	14.701248	-0.096437	4.597497
497.417338	7265.342925	14.706253	-0.096436	4.594978
497.843062	7257.340480	14.711258	-0.096510	4.592491
497.266927	7249.318060	14.716263	-0.096398	4.589996
497.920904	7241.252021	14.721267	-0.096514	4.587486
497.909610	7233.273225	14.726272	-0.096507	4.585002
497.188857	7225.416194	14.731277	-0.096367	4.582554
497.123277	7217.363290	14.736282	-0.096350	4.580044
497.364630	7209.342351	14.741287	-0.096390	4.577543
497.264918	7201.340454	14.746291	-0.096366	4.575046
497.233462	7193.313620	14.751296	-0.096355	4.572540
497.385337	7185.288201	14.756301	-0.096378	4.570033
497.632298	7177.311533	14.761306	-0.096419	4.567540
497.573171	7169.256093	14.766311	-0.096402	4.565021
497.109086	7161.391138	14.771315	-0.096311	4.562559
497.124881	7153.322229	14.776320	-0.096308	4.560033
497.248751	7145.348766	14.781325	-0.096326	4.557536
497.102272	7137.340602	14.786330	-0.096294	4.555026
497.128770	7129.342701	14.791335	-0.096294	4.552518
496.980180	7121.308657	14.796339	-0.096261	4.549997
496.778604	7113.338176	14.801344	-0.096218	4.547495
496.469878	7105.277575	14.806349	-0.096155	4.544962
496.346977	7097.389007	14.811354	-0.096127	4.542482
496.338951	7089.269659	14.816359	-0.096120	4.539929
496.567420	7081.291873	14.821363	-0.096158	4.537420
496.366461	7073.339793	14.826368	-0.096115	4.534916
496.031569	7065.315037	14.831373	-0.096047	4.532387
496.115434	7057.289315	14.836378	-0.096058	4.529858
495.923479	7049.264540	14.841383	-0.096017	4.527327
495.934780	7041.252400	14.846387	-0.096014	4.524799
495.822835	7033.287398	14.851392	-0.095988	4.522285
495.671119	7025.233382	14.856397	-0.095954	4.519740
495.842976	7017.307277	14.861402	-0.095981	4.517236
495.483978	7009.268307	14.866407	-0.095909	4.514693
495.858668	7001.280959	14.871411	-0.095973	4.512167
495.496172	6993.253181	14.876416	-0.095901	4.509624
495.124330	6985.291271	14.881421	-0.095826	4.507101
495.261341	6977.231112	14.886426	-0.095846	4.504547
495.127480	6969.255159	14.891431	-0.095816	4.502017
494.980677	6961.234708	14.896435	-0.095784	4.499472
495.307503	6953.209657	14.901440	-0.095839	4.496925
495.513132	6945.125555	14.906445	-0.095872	4.494358
495.344363	6937.228054	14.911450	-0.095836	4.491847
495.365575	6929.183638	14.916455	-0.095834	4.489289
495.658427	6921.194521	14.921459	-0.095884	4.486748
496.038802	6913.124456	14.926464	-0.095949	4.484180
495.675435	6905.256131	14.931469	-0.095876	4.481672
495.733080	6897.221616	14.936474	-0.095882	4.479111
495.513562	6889.272510	14.941479	-0.095836	4.476575
495.314243	6881.181030	14.946483	-0.095793	4.473993
495.151901	6873.273690	14.951488	-0.095758	4.471467
495.172630	6865.157437	14.956493	-0.095757	4.468874
495.129585	6857.193212	14.961498	-0.095743	4.466328
494.768184	6849.182278	14.966503	-0.095671	4.463765
494.415649	6841.257899	14.971507	-0.095600	4.461227
494.861885	6833.158332	14.976512	-0.095678	4.458635
494.937669	6825.121184	14.981517	-0.095687	4.456061
494.624342	6817.162426	14.986522	-0.095623	4.453508
495.036852	6809.117959	14.991527	-0.095695	4.450929
494.908971	6801.140466	14.996531	-0.095666	4.448368
495.037432	6793.127816	15.001536	-0.095684	4.445796
494.573385	6785.191910	15.006541	-0.095593	4.443244
494.974916	6777.215387	15.011546	-0.095662	4.440681
494.825193	6769.130639	15.016551	-0.095629	4.438080
494.103588	6761.247841	15.021555	-0.095490	4.435539
493.937656	6753.258248	15.026560	-0.095454	4.432964
493.859129	6745.177045	15.031565	-0.095434	4.430360
494.349487	6737.121321	15.036570	-0.095520	4.427765
494.717896	6729.012178	15.041575	-0.095583	4.425150
494.416377	6721.122914	15.046579	-0.095522	4.422602
494.317883	6713.132460	15.051584	-0.095498	4.420020
494.020556	6705.168480	15.056589	-0.095438	4.417445
494.485974	6697.097601	15.061594	-0.095519	4.414837
494.117157	6689.139504	15.066599	-0.095445	4.412260
493.981403	6681.135809	15.071603	-0.095415	4.409668
493.864195	6673.162561	15.076608	-0.095388	4.407084
493.640931	6665.116053	15.081613	-0.095341	4.404474
493.573398	6657.216856	15.086618	-0.095323	4.401912
493.583809	6649.099666	15.091623	-0.095320	4.399277
493.410630	6641.189724	15.096627	-0.095282	4.396708
493.933918	6633.082093	15.101632	-0.095374	4.394076
493.494796	6625.135730	15.106637	-0.095287	4.391490
493.333305	6617.194632	15.111642	-0.095252	4.388906
493.836141	6609.091929	15.116647	-0.095340	4.386271
493.901566	6601.050420	15.121651	-0.095347	4.383653
493.773601	6593.126717	15.126656	-0.095318	4.381070
493.713552	6585.170012	15.131661	-0.095302	4.378475
493.795177	6577.140577	15.136666	-0.095312	4.375855
493.851035	6569.137483	15.141671	-0.095317	4.373243
493.854629	6561.156478	15.146675	-0.095313	4.370636
493.820743	6553.135191	15.151680	-0.095301	4.368013
493.271358	6545.164892	15.156685	-0.095194	4.365403
493.427503	6537.221806	15.161690	-0.095217	4.362804
493.569643	6529.193152	15.166695	-0.095239	4.360176
493.516823	6521.222084	15.171699	-0.095224	4.357564
493.359882	6513.223824	15.176704	-0.095189	4.354941
493.668383	6505.149812	15.181709	-0.095241	4.352294
493.213548	6497.186915	15.186714	-0.095151	4.349677
492.443446	6489.222758	15.191719	-0.095003	4.347055
493.295359	6481.132121	15.196723	-0.095156	4.344403
492.942634	6473.232028	15.201728	-0.095085	4.341802
492.738356	6465.150350	15.206733	-0.095042	4.339141
492.569679	6457.241620	15.211738	-0.095005	4.336536
492.434240	6449.177792	15.216743	-0.094975	4.333878
492.465402	6441.194574	15.221747	-0.094976	4.331246
492.164906	6433.192858	15.226752	-0.094914	4.328605
492.283077	6425.171001	15.231757	-0.094931	4.325958
492.575936	6417.149795	15.236762	-0.094980	4.323311
492.312385	6409.191321	15.241767	-0.094926	4.320679
492.516891	6401.203677	15.246771	-0.094959	4.318039
492.415783	6393.226513	15.251776	-0.094935	4.315399
492.385674	6385.174267	15.256781	-0.094924	4.312733
492.380472	6377.161253	15.261786	-0.094918	4.310078
492.243483	6369.165935	15.266791	-0.094887	4.307427
492.090175	6361.132738	15.271795	-0.094853	4.304761
492.271047	6353.145838	15.276800	-0.094882	4.302111
491.898135	6345.145239	15.281805	-0.094807	4.299451
491.935631	6337.208544	15.286810	-0.094809	4.296814
491.516685	6329.186402	15.291815	-0.094726	4.294143
491.855090	6321.161573	15.296819	-0.094783	4.291476
492.181757	6313.077235	15.301824	-0.094839	4.288787
491.795593	6305.105053	15.306829	-0.094762	4.286128
491.989315	6297.114803	15.311834	-0.094793	4.283466
491.799724	6289.118374	15.316839	-0.094752	4.280797
491.692998	6281.174303	15.321843	-0.094727	4.278144
491.293991	6273.204037	15.326848	-0.094648	4.275479
491.643312	6265.129363	15.331853	-0.094707	4.272784
492.071005	6257.103186	15.336858	-0.094782	4.270104
491.759635	6249.079420	15.341863	-0.094719	4.267416
491.452928	6241.130622	15.346867	-0.094656	4.264752
491.335230	6233.207600	15.351872	-0.094629	4.262096
491.137144	6225.138276	15.356877	-0.094587	4.259389
491.289355	6217.151468	15.361882	-0.094610	4.256711
491.197282	6209.107958	15.366887	-0.094588	4.254010
491.188588	6201.164718	15.371891	-0.094581	4.251342
491.647717	6193.034343	15.376896	-0.094661	4.248614
491.669491	6185.068661	15.381901	-0.094660	4.245936
491.587598	6177.155628	15.386906	-0.094640	4.243272
491.017610	6169.188176	15.391911	-0.094528	4.240583
491.523402	6161.094253	15.396915	-0.094617	4.237861
491.469923	6153.087214	15.401920	-0.094602	4.235161
490.715326	6145.214173	15.406925	-0.094456	4.232497
490.186542	6137.196124	15.411930	-0.094353	4.229785
490.844162	6129.077215	15.416935	-0.094470	4.227049
490.793494	6121.060275	15.421939	-0.094455	4.224338
491.034230	6113.095609	15.426944	-0.094495	4.221647
490.784508	6105.078640	15.431949	-0.094443	4.218931
490.992362	6097.122377	15.436954	-0.094476	4.216238
490.977242	6089.053954	15.441959	-0.094468	4.213504
490.779467	6081.105279	15.446963	-0.094426	4.210806
491.102711	6073.100711	15.451968	-0.094481	4.208093
491.050921	6065.074835	15.456973	-0.094466	4.205367
490.563536	6057.175062	15.461978	-0.094370	4.202678
490.496005	6049.110619	15.466983	-0.094353	4.199935
490.796987	6041.163978	15.471987	-0.094403	4.197235
490.538176	6033.123721	15.476992	-0.094350	4.194495
490.518404	6025.067046	15.481997	-0.094341	4.191750
490.574373	6017.032327	15.487002	-0.094346	4.189011
490.398658	6009.068375	15.492007	-0.094308	4.186293
490.338862	6001.054504	15.497011	-0.094292	4.183557
490.252454	5993.129061	15.502016	-0.094271	4.180849
489.829798	5985.119080	15.507021	-0.094187	4.178106
489.699758	5977.144502	15.512026	-0.094157	4.175377
489.827252	5969.078636	15.517031	-0.094176	4.172618
489.503371	5961.111415	15.522035	-0.094110	4.169886
489.687223	5953.111545	15.527040	-0.094139	4.167147
489.562343	5945.025013	15.532045	-0.094111	4.164372
490.120083	5937.074116	15.537050	-0.094209	4.161651
489.707645	5929.094032	15.542055	-0.094127	4.158905
489.668247	5921.120431	15.547059	-0.094115	4.156165
489.887577	5913.089146	15.552064	-0.094150	4.153407
489.665816	5905.107364	15.557069	-0.094104	4.150658
489.296524	5897.120075	15.562074	-0.094030	4.147903
488.933772	5889.120799	15.567079	-0.093957	4.145143
489.259113	5881.145804	15.572083	-0.094012	4.142397
489.297945	5873.097104	15.577088	-0.094014	4.139621
489.375548	5865.093927	15.582093	-0.094024	4.136860
489.947879	5857.031325	15.587098	-0.094125	4.134082
489.428414	5849.135404	15.592103	-0.094023	4.131346
489.048726	5841.139454	15.597107	-0.093947	4.128575
489.277124	5833.122131	15.602112	-0.093984	4.125803
488.876497	5825.150551	15.607117	-0.093905	4.123037
488.831423	5817.167132	15.612122	-0.093891	4.120269
489.343503	5809.117941	15.617127	-0.093981	4.117484
489.047670	5801.146038	15.622131	-0.093921	4.114713
489.057814	5793.164918	15.627136	-0.093918	4.111942
488.525832	5785.132459	15.632141	-0.093813	4.109143
488.785444	5777.119165	15.637146	-0.093856	4.106360
488.679669	5769.068376	15.642151	-0.093831	4.103556
488.480094	5761.155052	15.647155	-0.093789	4.100798
488.930409	5753.102765	15.652160	-0.093868	4.097998
488.424832	5745.115946	15.657165	-0.093768	4.095206
488.388855	5737.153268	15.662170	-0.093756	4.092426
488.493879	5729.055310	15.667175	-0.093771	4.089600
488.183524	5721.130894	15.672179	-0.093708	4.086826
488.265338	5713.092296	15.677184	-0.093718	4.084017
488.065889	5705.187690	15.682189	-0.093675	4.081248
488.353703	5697.155960	15.687194	-0.093724	4.078439
487.765399	5689.167171	15.692199	-0.093609	4.075632
487.753096	5681.117223	15.697203	-0.093601	4.072809
487.768632	5673.122392	15.702208	-0.093599	4.070004
487.981032	5665.050068	15.707213	-0.093633	4.067172
487.927448	5657.072771	15.712218	-0.093618	4.064368
488.026527	5649.101579	15.717223	-0.093631	4.061567
487.913682	5641.094403	15.722227	-0.093605	4.058748
487.435565	5633.196360	15.727232	-0.093511	4.055959
487.568227	5625.091469	15.732237	-0.093530	4.053106
487.781979	5617.126781	15.737242	-0.093565	4.050301
487.459763	5609.162673	15.742247	-0.093500	4.047485
487.846778	5601.051993	15.747251	-0.093566	4.044628
488.137027	5593.088064	15.752256	-0.093615	4.041818
487.848856	5585.097829	15.757261	-0.093556	4.038988
487.441724	5577.248274	15.762266	-0.093476	4.036204
487.333186	5569.133593	15.767271	-0.093450	4.033329
487.736927	5561.034329	15.772275	-0.093520	4.030466
487.118717	5553.146943	15.777280	-0.093400	4.027659
486.860578	5545.079263	15.782285	-0.093346	4.024792
486.791732	5537.210978	15.787290	-0.093328	4.021997
487.383547	5529.030817	15.792295	-0.093433	4.019100
486.781218	5521.171766	15.797299	-0.093316	4.016295
486.812883	5513.134893	15.802304	-0.093317	4.013436
486.984413	5505.137583	15.807309	-0.093343	4.010591
486.713442	5497.203228	15.812314	-0.093288	4.007759
486.806067	5489.129865	15.817319	-0.093300	4.004881
486.552473	5481.230661	15.822323	-0.093247	4.002058
486.885203	5473.135652	15.827328	-0.093304	3.999173
486.768626	5465.176738	15.832333	-0.093277	3.996326
486.891393	5457.129295	15.837338	-0.093295	3.993450
486.444443	5449.188863	15.842343	-0.093206	3.990601
485.982740	5441.227120	15.847347	-0.093115	3.987742
486.420101	5433.103597	15.852352	-0.093191	3.984837
486.554653	5425.177053	15.857357	-0.093211	3.981997
486.440095	5417.195136	15.862362	-0.093184	3.979130
486.413059	5409.193052	15.867367	-0.093174	3.976255
486.455994	5401.124769	15.872371	-0.093177	3.973356
486.134753	5393.196464	15.877376	-0.093112	3.970498
485.839656	5385.179091	15.882381	-0.093052	3.967607
485.625970	5377.210456	15.887386	-0.093007	3.964732
485.925287	5369.200623	15.892391	-0.093057	3.961850
486.004714	5361.155539	15.897395	-0.093067	3.958949
485.723966	5353.244968	15.902400	-0.093009	3.956088
485.801355	5345.138292	15.907405	-0.093018	3.953161
485.822969	5337.158657	15.912410	-0.093017	3.950276
485.618835	5329.170383	15.917415	-0.092974	3.947382
485.402027	5321.150781	15.922419	-0.092928	3.944474
485.563984	5313.223835	15.927424	-0.092953	3.941605
485.093459	5305.207564	15.932429	-0.092860	3.938689
485.261561	5297.201639	15.937434	-0.092887	3.935787
485.173067	5289.168370	15.942439	-0.092865	3.932868
485.374073	5281.102954	15.947443	-0.092897	3.929940
485.406630	5273.155181	15.952448	-0.092898	3.927050
485.337852	5265.132788	15.957453	-0.092880	3.924129
485.290656	5257.231800	15.962458	-0.092866	3.921250
485.035522	5249.203719	15.967463	-0.092813	3.918319
484.712472	5241.253782	15.972467	-0.092748	3.915413
485.177555	5233.188716	15.977472	-0.092829	3.912477
484.982235	5225.152598	15.982477	-0.092787	3.909538
485.249455	5217.166267	15.987482	-0.092832	3.906623
485.477790	5209.106836	15.992487	-0.092869	3.903679
485.252214	5201.226902	15.997491	-0.092822	3.900789
485.250080	5193.220793	16.002496	-0.092816	3.897855
485.292848	5185.185102	16.007501	-0.092819	3.894909
484.952512	5177.293608	16.012506	-0.092751	3.892006
484.921053	5169.192503	16.017511	-0.092739	3.889030
484.812678	5161.270791	16.022515	-0.092714	3.886117
484.667935	5153.260342	16.027520	-0.092682	3.883167
484.602830	5145.236406	16.032525	-0.092665	3.880212
484.459325	5137.291566	16.037530	-0.092633	3.877283
484.620037	5129.241137	16.042535	-0.092657	3.874318
484.427720	5121.140306	16.047539	-0.092616	3.871325
484.579941	5113.090843	16.052544	-0.092639	3.868356
484.028272	5105.189098	16.057549	-0.092531	3.865425
484.284184	5097.244849	16.062554	-0.092574	3.862492
483.865768	5089.250936	16.067559	-0.092491	3.859525
483.957914	5081.239537	16.072563	-0.092503	3.856560
483.949579	5073.253440	16.077568	-0.092496	3.853600
483.932651	5065.207515	16.082573	-0.092487	3.850615
483.594765	5057.289586	16.087578	-0.092419	3.847668
483.699626	5049.223126	16.092583	-0.092434	3.844674
483.867276	5041.241557	16.097587	-0.092460	3.841710
483.768336	5033.243729	16.102592	-0.092436	3.838731
483.449334	5025.274960	16.107597	-0.092371	3.835757
483.831661	5017.275947	16.112602	-0.092437	3.832784
483.147237	5009.324261	16.117607	-0.092305	3.829804
483.177680	5001.277049	16.122611	-0.092305	3.826801
483.429839	4993.252374	16.127616	-0.092347	3.823809
483.732061	4985.190861	16.132621	-0.092398	3.820802
484.007038	4977.203909	16.137626	-0.092444	3.817819
484.055760	4969.188988	16.142631	-0.092448	3.814819
483.695741	4961.292111	16.147635	-0.092375	3.811852
483.131718	4953.342150	16.152640	-0.092265	3.808858
483.477952	4945.236111	16.157645	-0.092324	3.805824
483.236118	4937.345353	16.162650	-0.092274	3.802854
482.960325	4929.336727	16.167655	-0.092218	3.799838
483.207372	4921.305475	16.172659	-0.092258	3.796822
483.283426	4913.280926	16.177664	-0.092267	3.793802
483.119226	4905.275696	16.182669	-0.092232	3.790782
482.985470	4897.314788	16.187674	-0.092201	3.787777
482.679228	4889.307980	16.192679	-0.092139	3.784748
482.607449	4881.334633	16.197683	-0.092121	3.781734
483.158933	4873.240125	16.202688	-0.092218	3.778687
482.933041	4865.285739	16.207693	-0.092171	3.775673
483.065448	4857.298291	16.212698	-0.092190	3.772651
482.895461	4849.299758	16.217703	-0.092153	3.769617
482.979017	4841.317440	16.222707	-0.092164	3.766591
483.304805	4833.289348	16.227712	-0.092219	3.763552
483.456157	4825.278554	16.232717	-0.092242	3.760513
483.210109	4817.394421	16.237722	-0.092191	3.757510
483.298481	4809.308569	16.242727	-0.092202	3.754436
483.253051	4801.336951	16.247731	-0.092189	3.751399
482.978046	4793.372479	16.252736	-0.092132	3.748357
482.520550	4785.421321	16.257741	-0.092042	3.745314
482.705195	4777.419431	16.262746	-0.092071	3.742264
482.944132	4769.310227	16.267751	-0.092110	3.739172
482.645877	4761.431546	16.272755	-0.092049	3.736152
482.551039	4753.399448	16.277760	-0.092026	3.733076
482.840370	4745.338566	16.282765	-0.092075	3.729996
482.403076	4737.438854	16.287770	-0.091988	3.726958
482.085721	4729.418385	16.292775	-0.091924	3.723873
482.273811	4721.435113	16.297779	-0.091954	3.720813
482.247977	4713.418734	16.302784	-0.091944	3.717732
481.757374	4705.465511	16.307789	-0.091847	3.714662
481.834414	4697.413586	16.312794	-0.091856	3.711564
481.829629	4689.371329	16.317799	-0.091850	3.708467
481.604674	4681.373865	16.322803	-0.091803	3.705378
481.536177	4673.435864	16.327808	-0.091785	3.702313
481.690071	4665.372472	16.332813	-0.091809	3.699203
481.654441	4657.460081	16.337818	-0.091797	3.696144
481.353599	4649.437307	16.342823	-0.091736	3.693033
481.674291	4641.368364	16.347827	-0.091790	3.689918
481.725747	4633.410432	16.352832	-0.091794	3.686836
481.263265	4625.416631	16.357837	-0.091703	3.683724
481.459051	4617.450290	16.362842	-0.091734	3.680637
481.563944	4609.434871	16.367847	-0.091749	3.677526
481.103027	4601.472807	16.372851	-0.091658	3.674419
480.953171	4593.546141	16.377856	-0.091624	3.671330
481.120433	4585.450612	16.382861	-0.091650	3.668182
480.762942	4577.505343	16.387866	-0.091579	3.665076
480.656706	4569.511247	16.392871	-0.091554	3.661954
481.044555	4561.431498	16.397875	-0.091621	3.658810
481.082682	4553.494588	16.402880	-0.091622	3.655710
480.855838	4545.512613	16.407885	-0.091575	3.652582
481.017238	4537.475425	16.412890	-0.091600	3.649440
480.996388	4529.487311	16.417895	-0.091591	3.646310
480.569391	4521.549679	16.422899	-0.091506	3.643186
480.927461	4513.535212	16.427904	-0.091567	3.640050
480.529233	4505.581627	16.432909	-0.091488	3.636915
480.342543	4497.594724	16.437914	-0.091448	3.633770
480.364338	4489.518353	16.442919	-0.091447	3.630593
480.360272	4481.525373	16.447923	-0.091441	3.627445
480.457103	4473.507601	16.452928	-0.091454	3.624287
480.687084	4465.472230	16.457933	-0.091491	3.621124
480.669174	4457.527152	16.462938	-0.091483	3.617986
480.395249	4449.568690	16.467943	-0.091427	3.614833
480.594072	4441.528000	16.472947	-0.091458	3.611659
480.653841	4433.560313	16.477952	-0.091464	3.608506
480.015225	4425.604494	16.482957	-0.091340	3.605335
479.948880	4417.650585	16.487962	-0.091323	3.602179
480.033455	4409.571618	16.492967	-0.091333	3.598974
480.324772	4401.542052	16.497971	-0.091382	3.595793
480.412333	4393.568134	16.502976	-0.091393	3.592625
480.250476	4385.552101	16.507981	-0.091358	3.589430
480.280675	4377.589464	16.512986	-0.091358	3.586259
480.247168	4369.579863	16.517991	-0.091347	3.583064
480.121250	4361.610071	16.522995	-0.091318	3.579880
480.611669	4353.597009	16.528000	-0.091404	3.576694
480.322886	4345.602006	16.533005	-0.091345	3.573489
479.887846	4337.672016	16.538010	-0.091259	3.570303
479.976714	4329.654023	16.543015	-0.091270	3.567095
479.858687	4321.660279	16.548019	-0.091243	3.563887
479.942354	4313.706075	16.553024	-0.091253	3.560698
479.587540	4305.714303	16.558029	-0.091182	3.557478
480.202957	4297.602274	16.563034	-0.091291	3.554236
480.123760	4289.592654	16.568039	-0.091271	3.551011
479.830614	4281.616676	16.573043	-0.091212	3.547791
479.931477	4273.629692	16.578048	-0.091225	3.544575
479.476423	4265.744181	16.583053	-0.091135	3.541380
479.593346	4257.719436	16.588058	-0.091152	3.538143
479.566128	4249.694514	16.593063	-0.091142	3.534899
478.953818	4241.782925	16.598067	-0.091022	3.531680
479.480533	4233.669226	16.603072	-0.091115	3.528411
479.759301	4225.632028	16.608077	-0.091162	3.525163
479.254511	4217.779778	16.613082	-0.091063	3.521962
479.523505	4209.705691	16.618087	-0.091107	3.518692
479.723060	4201.710437	16.623091	-0.091139	3.515449
479.696212	4193.759332	16.628096	-0.091129	3.512214
479.524758	4185.715751	16.633101	-0.091092	3.508934
479.333021	4177.808482	16.638106	-0.091051	3.505705
479.552304	4169.760737	16.643111	-0.091087	3.502430
478.968309	4161.828099	16.648115	-0.090973	3.499172
478.743325	4153.913686	16.653120	-0.090926	3.495931
478.604798	4145.819068	16.658125	-0.090895	3.492615
478.407002	4137.831421	16.663130	-0.090853	3.489338
478.182947	4129.876309	16.668135	-0.090806	3.486071
477.947629	4121.860438	16.673139	-0.090757	3.482775
478.135124	4113.852633	16.678144	-0.090786	3.479493
478.295056	4105.815790	16.683149	-0.090811	3.476195
477.761881	4097.944643	16.688154	-0.090706	3.472940
477.682182	4089.853602	16.693159	-0.090686	3.469605
477.537213	4081.877863	16.698163	-0.090654	3.466313
478.145687	4073.788238	16.703168	-0.090762	3.462996
477.697928	4065.854559	16.708173	-0.090674	3.459705
477.443729	4057.918931	16.713178	-0.090621	3.456416
477.570547	4049.896542	16.718183	-0.090639	3.453101
477.550309	4041.868209	16.723187	-0.090630	3.449775
477.611509	4033.865798	16.728192	-0.090637	3.446460
477.400170	4025.915263	16.733197	-0.090592	3.443154
477.484100	4017.930873	16.738202	-0.090602	3.439841
476.912059	4010.011290	16.743207	-0.090491	3.436529
477.082831	4001.945924	16.748211	-0.090517	3.433178
477.432414	3993.901244	16.753216	-0.090577	3.429839
477.501576	3985.884555	16.758221	-0.090585	3.426499
477.457318	3977.937443	16.763226	-0.090571	3.423180
477.164382	3969.976255	16.768231	-0.090512	3.419844
476.925445	3962.006518	16.773235	-0.090462	3.416503
477.067426	3953.993353	16.778240	-0.090483	3.413154
477.341848	3945.910573	16.783245	-0.090529	3.409777
477.238953	3937.979822	16.788250	-0.090504	3.406447
477.881853	3929.874951	16.793255	-0.090619	3.403067
477.850236	3921.953754	16.798259	-0.090608	3.399737
477.253829	3914.124617	16.803264	-0.090492	3.396422
477.309790	3906.032263	16.808269	-0.090497	3.393017
476.773079	3898.078496	16.813274	-0.090392	3.389645
476.483738	3890.108066	16.818279	-0.090333	3.386272
476.402026	3882.098383	16.823283	-0.090312	3.382886
477.103481	3873.970489	16.828288	-0.090437	3.379475
476.989834	3865.998020	16.833293	-0.090411	3.376097
476.666990	3858.093614	16.838298	-0.090346	3.372737
476.341811	3850.123120	16.843303	-0.090280	3.369345
476.770546	3842.038906	16.848307	-0.090355	3.365929
476.511133	3834.140672	16.853312	-0.090301	3.362564
476.152460	3826.158598	16.858317	-0.090229	3.359156
476.025356	3818.228371	16.863322	-0.090200	3.355774
475.675567	3810.223159	16.868327	-0.090130	3.352350
475.928124	3802.129661	16.873331	-0.090172	3.348906
475.616626	3794.187405	16.878336	-0.090108	3.345502
475.828561	3786.143106	16.883341	-0.090143	3.342071
476.130761	3778.117971	16.888346	-0.090194	3.338648
475.901662	3770.196673	16.893351	-0.090146	3.335246
475.855522	3762.203336	16.898355	-0.090132	3.331817
475.740769	3754.232341	16.903360	-0.090105	3.328391
475.842139	3746.160347	16.908365	-0.090119	3.324926
475.829137	3738.235313	16.913370	-0.090111	3.321516
476.010575	3730.191635	16.918375	-0.090140	3.318060
475.502193	3722.302704	16.923379	-0.090040	3.314640
475.669913	3714.286301	16.928384	-0.090066	3.311187
475.509484	3706.251340	16.933389	-0.090031	3.307710
475.387590	3698.269786	16.938394	-0.090003	3.304254
475.162431	3690.330478	16.943399	-0.089956	3.300809
475.219759	3682.296960	16.948403	-0.089961	3.297330
475.098742	3674.349212	16.953408	-0.089934	3.293877
475.162048	3666.298975	16.958413	-0.089940	3.290384
475.246753	3658.302686	16.963418	-0.089951	3.286912
475.074343	3650.337560	16.968423	-0.089913	3.283439
475.090840	3642.337884	16.973427	-0.089911	3.279954
474.890768	3634.416641	16.978432	-0.089869	3.276492
475.116833	3626.332499	16.983437	-0.089906	3.272972
474.690847	3618.435486	16.988442	-0.089821	3.269504
474.872382	3610.379051	16.993447	-0.089850	3.265987
474.541137	3602.449851	16.998451	-0.089783	3.262501
474.368116	3594.479763	17.003456	-0.089745	3.258999
474.432830	3586.461426	17.008461	-0.089752	3.255483
474.653357	3578.432263	17.013466	-0.089788	3.251964
474.621046	3570.425320	17.018471	-0.089777	3.248441
474.341825	3562.467858	17.023475	-0.089720	3.244925
474.632527	3554.494136	17.028480	-0.089769	3.241422
474.190539	3546.528313	17.033485	-0.089681	3.237889
474.657715	3538.464070	17.038490	-0.089763	3.234346
474.897578	3530.449600	17.043495	-0.089802	3.230811
474.104542	3522.570853	17.048499	-0.089649	3.227290
474.185040	3514.534020	17.053504	-0.089659	3.223731
473.897981	3506.570386	17.058509	-0.089600	3.220186
473.699396	3498.598838	17.063514	-0.089558	3.216636
473.850372	3490.530664	17.068519	-0.089581	3.213055
473.748672	3482.557880	17.073523	-0.089557	3.209501
473.952821	3474.567564	17.078528	-0.089590	3.205948
474.112239	3466.512665	17.083533	-0.089614	3.202361
474.204446	3458.543714	17.088538	-0.089626	3.198805
473.911196	3450.642257	17.093543	-0.089566	3.195260
473.915730	3442.617192	17.098547	-0.089562	3.191667
473.836111	3434.653144	17.103552	-0.089542	3.188094
473.854955	3426.626655	17.108557	-0.089540	3.184494
473.397358	3418.749169	17.113562	-0.089450	3.180935
473.473046	3410.724189	17.118567	-0.089459	3.177330
473.464986	3402.689402	17.123571	-0.089452	3.173712
473.620076	3394.688726	17.128576	-0.089476	3.170112
473.485609	3386.691457	17.133581	-0.089445	3.166498
473.849545	3378.677414	17.138586	-0.089508	3.162893
473.407639	3370.807905	17.143591	-0.089420	3.159315
473.061485	3362.871975	17.148595	-0.089351	3.155706
473.495830	3354.786567	17.153600	-0.089426	3.152060
473.397711	3346.733936	17.158605	-0.089403	3.148401
473.756247	3338.706024	17.163610	-0.089464	3.144770
473.450113	3330.818180	17.168615	-0.089402	3.141168
473.518463	3322.779065	17.173619	-0.089410	3.137510
473.340842	3314.880498	17.178624	-0.089371	3.133900
472.873544	3306.900352	17.183629	-0.089279	3.130236
473.202985	3298.846872	17.188634	-0.089335	3.126571
472.922684	3290.928418	17.193639	-0.089278	3.122935
473.014057	3282.898318	17.198643	-0.089290	3.119261
472.808485	3274.991801	17.203648	-0.089246	3.115625
472.816849	3266.935160	17.208653	-0.089243	3.111926
472.840089	3258.940216	17.213658	-0.089242	3.108252
472.716241	3250.977700	17.218663	-0.089213	3.104581
473.064895	3242.928803	17.223667	-0.089273	3.100889
472.906200	3234.997539	17.228672	-0.089238	3.097222
472.641829	3227.033789	17.233677	-0.089184	3.093531
472.927999	3218.992644	17.238682	-0.089232	3.089826
473.003020	3211.008802	17.243687	-0.089241	3.086133
472.812228	3203.025947	17.248691	-0.089200	3.082423
472.289081	3195.164112	17.253696	-0.089097	3.078750
471.978456	3187.182043	17.258701	-0.089034	3.075026
471.969125	3179.121191	17.263706	-0.089027	3.071275
471.732931	3171.131042	17.268711	-0.088978	3.067542
471.531654	3163.135104	17.273715	-0.088935	3.063803
471.722872	3155.156606	17.278720	-0.088966	3.060086
471.856290	3147.134958	17.283725	-0.088985	3.056343
471.392041	3139.211687	17.288730	-0.088894	3.052611
471.655351	3131.144897	17.293735	-0.088938	3.048843
471.848476	3123.130487	17.298739	-0.088968	3.045092
471.898854	3115.181245	17.303744	-0.088972	3.041359
472.136031	3107.140648	17.308749	-0.089011	3.037589
472.358469	3099.164452	17.313754	-0.089048	3.033843
472.224499	3091.204917	17.318759	-0.089017	3.030083
471.924081	3083.255630	17.323763	-0.088956	3.026315
472.307654	3075.245104	17.328768	-0.089022	3.022547
471.658478	3067.372332	17.333773	-0.088896	3.018788
471.388278	3059.412414	17.338778	-0.088841	3.015002
471.329162	3051.414008	17.343783	-0.088825	3.011203
471.515189	3043.346559	17.348787	-0.088854	3.007379
471.668720	3035.341911	17.353792	-0.088877	3.003579
471.323385	3027.411512	17.358797	-0.088808	2.999784
471.293474	3019.481923	17.363802	-0.088797	2.996000
470.895764	3011.515392	17.368807	-0.088718	2.992175
470.990300	3003.449848	17.373811	-0.088730	2.988323
471.003648	2995.451575	17.378816	-0.088728	2.984495
471.323880	2987.409144	17.383821	-0.088782	2.980656
471.144959	2979.492978	17.388826	-0.088743	2.976846
471.017010	2971.534810	17.393831	-0.088714	2.973015
470.991869	2963.485116	17.398835	-0.088704	2.969139
470.806314	2955.577884	17.403840	-0.088665	2.965319
470.697430	2947.591811	17.408845	-0.088639	2.961460
470.906469	2939.581715	17.413850	-0.088673	2.957601
470.681562	2931.630417	17.418855	-0.088626	2.953743
470.684478	2923.618450	17.423859	-0.088621	2.949862
470.812145	2915.652948	17.428864	-0.088640	2.946005
470.720720	2907.663936	17.433869	-0.088617	2.942120
470.882160	2899.645017	17.438874	-0.088642	2.938228
470.321956	2891.756770	17.443879	-0.088533	2.934357
470.389029	2883.738026	17.448883	-0.088540	2.930451
470.067151	2875.812356	17.453888	-0.088475	2.926563
470.510105	2867.722467	17.458893	-0.088552	2.922632
470.374978	2859.809023	17.463898	-0.088522	2.918750
470.478820	2851.824377	17.468903	-0.088536	2.914842
470.033682	2843.815253	17.473907	-0.088448	2.910886
470.213064	2835.775221	17.478912	-0.088476	2.906943
470.149540	2827.808506	17.483917	-0.088459	2.903018
469.919528	2819.863549	17.488922	-0.088411	2.899089
470.431740	2811.806841	17.493927	-0.088501	2.895141
470.178781	2803.876048	17.498931	-0.088449	2.891207
470.340348	2795.880772	17.503936	-0.088474	2.887259
470.308793	2787.882124	17.508941	-0.088463	2.883293
470.487532	2779.906075	17.513946	-0.088491	2.879345
470.011170	2772.060431	17.518951	-0.088397	2.875419
469.784122	2764.062234	17.523955	-0.088349	2.871426
470.017593	2756.032666	17.528960	-0.088387	2.867438
470.139476	2748.013013	17.533965	-0.088405	2.863443
469.489762	2740.144370	17.538970	-0.088279	2.859474
469.404005	2732.182461	17.543975	-0.088258	2.855484
469.690043	2724.104159	17.548979	-0.088306	2.851452
469.818034	2716.135945	17.553984	-0.088324	2.847461
468.901225	2708.275698	17.558989	-0.088148	2.843458
468.822812	2700.296480	17.563994	-0.088129	2.839438
469.143361	2692.253217	17.568999	-0.088183	2.835403
468.822497	2684.292312	17.574003	-0.088118	2.831366
468.879886	2676.271090	17.579008	-0.088124	2.827316
468.679658	2668.289743	17.584013	-0.088081	2.823264
468.865211	2660.282881	17.589018	-0.088110	2.819216
469.236976	2652.262844	17.594023	-0.088174	2.815167
468.751611	2644.369836	17.599027	-0.088079	2.811126
468.866347	2636.356418	17.604032	-0.088095	2.807054
468.203448	2628.482127	17.609037	-0.087966	2.803000
468.175374	2620.492036	17.614042	-0.087956	2.798919
468.321868	2612.476816	17.619047	-0.087978	2.794830
468.264622	2604.453138	17.624051	-0.087962	2.790718
468.606406	2596.420865	17.629056	-0.088020	2.786619
468.502924	2588.463249	17.634061	-0.087996	2.782526
468.828299	2580.463498	17.639066	-0.088051	2.778431
468.880468	2572.496528	17.644071	-0.088056	2.774331
468.537111	2564.569668	17.649075	-0.087987	2.770221
468.787432	2556.561291	17.654080	-0.088028	2.766099
468.540508	2548.613118	17.659085	-0.087977	2.761972
468.551325	2540.679020	17.664090	-0.087974	2.757861
468.464596	2532.695546	17.669095	-0.087952	2.753713
468.496299	2524.632676	17.674099	-0.087953	2.749525
468.554623	2516.658624	17.679104	-0.087959	2.745378
468.285095	2508.746350	17.684109	-0.087903	2.741236
467.895407	2500.837792	17.689114	-0.087826	2.737083
467.917651	2492.827870	17.694119	-0.087824	2.732896
467.857709	2484.825734	17.699123	-0.087808	2.728702
467.997517	2476.819755	17.704128	-0.087829	2.724511
467.327711	2468.972969	17.709133	-0.087699	2.720347
467.321851	2460.998360	17.714138	-0.087693	2.716151
467.756334	2452.918576	17.719143	-0.087768	2.711921
467.610480	2444.941164	17.724147	-0.087736	2.707702
468.078158	2436.883344	17.729152	-0.087818	2.703473
467.499212	2429.020345	17.734157	-0.087705	2.699273
467.378491	2421.077962	17.739162	-0.087677	2.695054
467.094906	2413.139636	17.744167	-0.087619	2.690820
466.554991	2405.188209	17.749171	-0.087513	2.686555
467.389817	2397.084247	17.754176	-0.087664	2.682292
466.565302	2389.262079	17.759181	-0.087505	2.678064
466.634251	2381.246233	17.764186	-0.087513	2.673785
466.686904	2373.245753	17.769191	-0.087517	2.669505
466.758030	2365.206935	17.774195	-0.087525	2.665200
466.993074	2357.221955	17.779200	-0.087564	2.660927
466.741301	2349.296683	17.784205	-0.087512	2.656648
466.744787	2341.331508	17.789210	-0.087507	2.652356
466.963315	2333.289719	17.794215	-0.087542	2.648031
466.399813	2325.415424	17.799219	-0.087432	2.643737
466.690620	2317.396824	17.804224	-0.087481	2.639415
466.140017	2309.520055	17.809229	-0.087374	2.635107
465.992811	2301.539581	17.814234	-0.087341	2.630762
466.497554	2293.461047	17.819239	-0.087430	2.626400
466.180807	2285.551295	17.824243	-0.087366	2.622068
465.713943	2277.671780	17.829248	-0.087274	2.617735
465.594822	2269.661237	17.834253	-0.087246	2.613347
465.778006	2261.627874	17.839258	-0.087275	2.608959
465.710885	2253.640935	17.844263	-0.087257	2.604572
465.655853	2245.703149	17.849267	-0.087242	2.600206
465.808547	2237.743022	17.854272	-0.087265	2.595834
465.780385	2229.672998	17.859277	-0.087255	2.591382
465.457738	2221.712658	17.864282	-0.087189	2.586963
465.309597	2213.774831	17.869287	-0.087156	2.582560
465.430490	2205.768815	17.874291	-0.087174	2.578131
465.543004	2197.806191	17.879296	-0.087189	2.573717
465.279841	2189.856786	17.884301	-0.087135	2.569277
465.423185	2181.873347	17.889306	-0.087157	2.564840
465.322532	2173.945812	17.894311	-0.087133	2.560408
465.172484	2165.999009	17.899315	-0.087100	2.555954
465.722397	2157.964133	17.904320	-0.087197	2.551493
465.425126	2150.014123	17.909325	-0.087136	2.547012
465.421030	2142.044414	17.914330	-0.087130	2.542532
465.732369	2134.042828	17.919335	-0.087183	2.538049
464.940818	2126.218978	17.924339	-0.087031	2.533579
464.927925	2118.247605	17.929344	-0.087023	2.529074
465.105689	2110.220734	17.934349	-0.087051	2.524544
465.427901	2102.226408	17.939354	-0.087106	2.520034
465.236162	2094.319890	17.944359	-0.087065	2.515528
464.736056	2086.416782	17.949363	-0.086966	2.510994
464.922709	2078.395096	17.954368	-0.086996	2.506434
465.206108	2070.352141	17.959373	-0.087043	2.501861
464.828630	2062.458517	17.964378	-0.086968	2.497316
464.970549	2054.492954	17.969383	-0.086989	2.492761
464.692039	2046.527054	17.974387	-0.086932	2.488165
464.835066	2038.529502	17.979392	-0.086954	2.483574
464.768797	2030.583699	17.984397	-0.086936	2.478989
464.600205	2022.665467	17.989402	-0.086899	2.474403
464.533616	2014.706340	17.994407	-0.086882	2.469793
464.340702	2006.731051	17.999411	-0.086841	2.465155
464.086044	1998.836725	18.004416	-0.086788	2.460551
464.526165	1990.777792	18.009421	-0.086865	2.455896
464.419249	1982.813379	18.014426	-0.086840	2.451244
463.867905	1974.938504	18.019431	-0.086732	2.446602
463.900708	1966.950603	18.024435	-0.086733	2.441931
464.112198	1958.973477	18.029440	-0.086767	2.437270
463.889782	1950.999119	18.034445	-0.086720	2.432568
464.356374	1942.937260	18.039450	-0.086802	2.427860
464.072915	1935.037969	18.044455	-0.086744	2.423179
463.877463	1927.084339	18.049459	-0.086702	2.418464
463.683267	1919.175937	18.054464	-0.086661	2.413767
463.948439	1911.146041	18.059469	-0.086705	2.409025
463.207642	1903.297407	18.064474	-0.086562	2.404301
463.542081	1895.297753	18.069479	-0.086619	2.399564
463.494291	1887.326731	18.074483	-0.086605	2.394804
463.402488	1879.385832	18.079488	-0.086583	2.390049
463.079263	1871.440606	18.084493	-0.086517	2.385263
462.901431	1863.497676	18.089498	-0.086479	2.380480
463.298504	1855.477522	18.094503	-0.086548	2.375688
462.607510	1847.621419	18.099507	-0.086414	2.370897
462.853274	1839.597454	18.104512	-0.086455	2.366071
462.966226	1831.629566	18.109517	-0.086470	2.361258
463.115434	1823.647723	18.114522	-0.086493	2.356430
462.655014	1815.783094	18.119527	-0.086402	2.351613
463.005068	1807.708444	18.124531	-0.086462	2.346726
462.465973	1799.882058	18.129536	-0.086357	2.341905
462.326905	1791.912021	18.134541	-0.086325	2.337021
462.434444	1783.903944	18.139546	-0.086340	2.332123
462.980552	1775.848338	18.144551	-0.086437	2.327222
462.728294	1767.956875	18.149555	-0.086384	2.322345
462.644237	1760.048216	18.154560	-0.086364	2.317462
462.445299	1752.117279	18.159565	-0.086321	2.312544
462.168303	1744.182840	18.164570	-0.086265	2.307608
461.905683	1736.272874	18.169575	-0.086211	2.302677
462.021016	1728.268492	18.174579	-0.086227	2.297709
461.964982	1720.332507	18.179584	-0.086211	2.292758
461.855938	1712.362350	18.184589	-0.086186	2.287770
461.548227	1704.460802	18.189594	-0.086123	2.282797
461.470739	1696.531581	18.194599	-0.086104	2.277816
461.473358	1688.529756	18.199603	-0.086099	2.272786
461.540519	1680.515873	18.204608	-0.086106	2.267742
461.713246	1672.520866	18.209613	-0.086133	2.262708
461.578584	1664.609276	18.214618	-0.086103	2.257689
461.246358	1656.721060	18.219623	-0.086036	2.252656
461.259870	1648.750613	18.224627	-0.086033	2.247590
461.337348	1640.798214	18.229632	-0.086042	2.242529
460.846206	1632.908971	18.234637	-0.085946	2.237447
460.933031	1624.935669	18.239642	-0.085957	2.232351
460.945807	1616.980940	18.244647	-0.085954	2.227249
460.598650	1609.076887	18.249651	-0.085884	2.222135
460.527525	1601.141229	18.254656	-0.085866	2.217014
460.631675	1593.143212	18.259661	-0.085880	2.211856
460.801678	1585.147951	18.264666	-0.085906	2.206695
460.787211	1577.222347	18.269671	-0.085898	2.201549
460.763856	1569.291121	18.274675	-0.085889	2.196388
461.469172	1561.227803	18.279680	-0.086015	2.191195
460.611906	1553.436586	18.284685	-0.085850	2.186022
461.225540	1545.369936	18.289690	-0.085959	2.180794
461.188577	1537.479194	18.294695	-0.085947	2.175609
461.148826	1529.531888	18.299699	-0.085935	2.170373
460.480537	1521.700649	18.304704	-0.085805	2.165142
460.495519	1513.759483	18.309709	-0.085803	2.159890
460.549954	1505.818550	18.314714	-0.085808	2.154629
460.855524	1497.788698	18.319719	-0.085859	2.149320
460.435802	1489.898287	18.324723	-0.085776	2.144021
460.742277	1481.939334	18.329728	-0.085828	2.138734
460.639934	1474.015393	18.334733	-0.085804	2.133417
460.964763	1466.006936	18.339738	-0.085859	2.128071
460.737696	1458.148987	18.344743	-0.085811	2.122760
460.083555	1450.332401	18.349747	-0.085684	2.117422
459.882540	1442.396417	18.354752	-0.085642	2.112033
460.158302	1434.334925	18.359757	-0.085688	2.106593
459.972454	1426.421563	18.364762	-0.085648	2.101194
459.667563	1418.552825	18.369767	-0.085586	2.095799
459.386965	1410.629403	18.374771	-0.085529	2.090355
459.721321	1402.608752	18.379776	-0.085586	2.084892
459.485983	1394.718302	18.384781	-0.085537	2.079447
459.797392	1386.726919	18.389786	-0.085590	2.073973
460.494005	1378.680149	18.394791	-0.085714	2.068485
459.954815	1370.850760	18.399795	-0.085609	2.063008
459.503686	1363.026494	18.404800	-0.085519	2.057529
459.201293	1355.117586	18.409805	-0.085458	2.051992
459.250772	1347.155709	18.414810	-0.085462	2.046438
459.236395	1339.234139	18.419815	-0.085454	2.040891
458.774990	1331.366703	18.424819	-0.085363	2.035321
459.119204	1323.358779	18.429824	-0.085422	2.029720
458.409326	1315.538672	18.434829	-0.085285	2.024126
458.601484	1307.545951	18.439834	-0.085315	2.018488
458.708842	1299.604640	18.444839	-0.085330	2.012863
458.172217	1291.745964	18.449843	-0.085225	2.007213
458.219963	1283.785188	18.454848	-0.085229	2.001535
458.211382	1275.854445	18.459853	-0.085222	1.995857
458.392239	1267.886754	18.464858	-0.085250	1.990157
457.957052	1260.028867	18.469863	-0.085164	1.984453
457.813616	1252.123973	18.474867	-0.085132	1.978730
457.741948	1244.208699	18.479872	-0.085114	1.972991
457.554029	1236.288396	18.484877	-0.085074	1.967218
457.737388	1228.309677	18.489882	-0.085103	1.961427
457.764525	1220.413645	18.494887	-0.085102	1.955662
457.743561	1212.458089	18.499891	-0.085093	1.949830
457.897373	1204.507854	18.504896	-0.085117	1.944005
457.522833	1196.657971	18.509901	-0.085042	1.938177
457.954389	1188.635897	18.514906	-0.085117	1.932294
458.377695	1180.650873	18.519911	-0.085191	1.926420
458.054772	1172.814041	18.524915	-0.085125	1.920555
457.752867	1164.990268	18.529920	-0.085064	1.914683
457.744554	1157.072875	18.534925	-0.085057	1.908757
457.374263	1149.206583	18.539930	-0.084983	1.902809
457.988402	1141.190006	18.544935	-0.085092	1.896842
457.824167	1133.299488	18.549939	-0.085057	1.890862
457.866193	1125.386141	18.554944	-0.085059	1.884869
457.386493	1117.595976	18.559949	-0.084965	1.878891
457.125348	1109.713805	18.564954	-0.084911	1.872848
456.983462	1101.815185	18.569959	-0.084879	1.866787
456.923447	1093.878803	18.574963	-0.084863	1.860687
457.692408	1085.850389	18.579968	-0.085001	1.854595
456.833812	1078.094817	18.584973	-0.084836	1.848499
456.634235	1070.181983	18.589978	-0.084794	1.842341
456.538060	1062.307269	18.594983	-0.084771	1.836203
457.115365	1054.275830	18.599987	-0.084873	1.830003
456.981702	1046.408055	18.604992	-0.084843	1.823825
456.899160	1038.530561	18.609997	-0.084822	1.817625
456.883389	1030.633285	18.615002	-0.084814	1.811395
456.837296	1022.746181	18.620007	-0.084801	1.805149
456.575288	1014.901031	18.625011	-0.084747	1.798887
457.214681	1006.884710	18.630016	-0.084860	1.792579
456.625333	999.074588	18.635021	-0.084746	1.786261
456.763788	991.140827	18.640026	-0.084766	1.779912
456.802966	983.277570	18.645031	-0.084768	1.773584
456.373971	975.446733	18.650035	-0.084683	1.767201
456.616928	967.521473	18.655040	-0.084723	1.760803
456.172313	959.722180	18.660045	-0.084636	1.754397
456.012316	951.848615	18.665050	-0.084601	1.747943
456.292427	943.906701	18.670055	-0.084648	1.741466
455.744650	936.105481	18.675059	-0.084541	1.734973
455.967408	928.172620	18.680064	-0.084577	1.728447
455.856353	920.297767	18.685069	-0.084551	1.721901
455.527803	912.481955	18.690074	-0.084485	1.715351
455.392283	904.621064	18.695079	-0.084454	1.708763
455.301010	896.723041	18.700083	-0.084432	1.702124
455.046613	888.873900	18.705088	-0.084380	1.695479
455.520171	880.887558	18.710093	-0.084463	1.688789
455.132496	873.092748	18.715098	-0.084385	1.682119
455.222451	865.213329	18.720103	-0.084397	1.675415
454.947786	857.376288	18.725107	-0.084341	1.668670
454.710356	849.544917	18.730112	-0.084291	1.661909
454.528097	841.699254	18.735117	-0.084252	1.655114
454.498467	833.809257	18.740122	-0.084242	1.648275
454.760612	825.895525	18.745127	-0.084285	1.641426
454.768129	818.036293	18.750131	-0.084282	1.634562
454.946898	810.111385	18.755136	-0.084310	1.627634
454.627179	802.302508	18.760141	-0.084245	1.620709
454.970616	794.381774	18.765146	-0.084304	1.613749
455.006628	786.539781	18.770151	-0.084305	1.606786
454.781949	778.733119	18.775155	-0.084258	1.599786
454.682721	770.922171	18.780160	-0.084235	1.592769
454.515286	763.092670	18.785165	-0.084199	1.585695
454.377539	755.284294	18.790170	-0.084168	1.578613
454.089746	747.485399	18.795175	-0.084109	1.571485
453.723671	739.687013	18.800179	-0.084036	1.564314
453.993067	731.797483	18.805184	-0.084081	1.557120
453.755903	723.980027	18.810189	-0.084032	1.549883
453.872351	716.106174	18.815194	-0.084048	1.542614
453.363840	708.373828	18.820199	-0.083948	1.535347
453.258118	700.532355	18.825203	-0.083924	1.528004
453.056520	692.725317	18.830208	-0.083881	1.520644
453.467489	684.806769	18.835213	-0.083952	1.513237
453.122023	677.033368	18.840218	-0.083883	1.505815
453.210777	669.205216	18.845223	-0.083894	1.498371
453.715345	661.266218	18.850227	-0.083983	1.490848
453.331681	653.560534	18.855232	-0.083907	1.483373
453.019212	645.813312	18.860237	-0.083843	1.475830
452.805388	637.988870	18.865242	-0.083798	1.468189
453.346675	630.075715	18.870247	-0.083894	1.460543
453.068832	622.323509	18.875251	-0.083837	1.452882
452.908451	614.544510	18.880256	-0.083802	1.445174
452.557170	606.830769	18.885261	-0.083732	1.437457
452.640978	598.993327	18.890266	-0.083742	1.429647
452.797381	591.171282	18.895271	-0.083766	1.421821
452.618758	583.416918	18.900275	-0.083728	1.413965
452.487706	575.656464	18.905280	-0.083698	1.406067
452.211726	567.925895	18.910285	-0.083642	1.398129
452.307517	560.107938	18.915290	-0.083655	1.390120
452.579342	552.280621	18.920295	-0.083700	1.382085
452.151572	544.593994	18.925299	-0.083616	1.374029
451.968741	536.851864	18.930304	-0.083577	1.365909
451.707119	529.150666	18.935309	-0.083523	1.357771
451.935152	521.319832	18.940314	-0.083560	1.349532
451.843785	513.583492	18.945319	-0.083538	1.341286
451.370871	505.913091	18.950323	-0.083445	1.332992
451.864068	498.056802	18.955328	-0.083532	1.324619
451.970228	490.308035	18.960333	-0.083546	1.316240
451.840517	482.508995	18.965338	-0.083517	1.307709
451.371962	474.872995	18.970343	-0.083425	1.299239
451.216836	467.156888	18.975347	-0.083391	1.290682
451.171450	459.442250	18.980352	-0.083377	1.282091
451.321654	451.706962	18.985357	-0.083400	1.273455
451.053507	444.028828	18.990362	-0.083345	1.264745
450.766307	436.382440	18.995367	-0.083287	1.256008
450.727104	428.660322	19.000371	-0.083275	1.247170
451.024986	420.918032	19.005376	-0.083325	1.238312
450.641505	413.294815	19.010381	-0.083249	1.229394
450.236753	405.670966	19.015386	-0.083168	1.220405
450.445736	397.953687	19.020391	-0.083202	1.211363
449.942545	390.355723	19.025395	-0.083103	1.202251
450.242997	382.627584	19.030400	-0.083154	1.193077
450.939056	374.829116	19.035405	-0.083279	1.183828
450.592099	367.264496	19.040410	-0.083209	1.174575
450.530681	359.639199	19.045415	-0.083193	1.165234
450.035204	352.097779	19.050419	-0.083096	1.155829
449.884314	344.466589	19.055424	-0.083063	1.146308
449.894163	336.831545	19.060429	-0.083059	1.136737
449.625316	329.248568	19.065434	-0.083004	1.127091
449.570372	321.667494	19.070439	-0.082989	1.117410
449.397707	314.089616	19.075443	-0.082952	1.107623
449.248752	306.519157	19.080448	-0.082920	1.097763
449.121995	298.953827	19.085453	-0.082891	1.087826
448.308079	291.531528	19.090458	-0.082735	1.077829
448.301789	283.956898	19.095463	-0.082728	1.067722
448.726398	276.295476	19.100467	-0.082802	1.057501
448.091435	268.868046	19.105472	-0.082679	1.047249
447.834415	261.379025	19.110477	-0.082627	1.036902
447.741652	253.854399	19.115482	-0.082604	1.026440
447.600146	246.371322	19.120487	-0.082573	1.015917
447.245149	238.918331	19.125491	-0.082502	1.005273
447.120606	231.454164	19.130496	-0.082474	0.994557
447.175765	223.927804	19.135501	-0.082480	0.983680
447.079381	216.472190	19.140506	-0.082457	0.972746
446.898798	209.060729	19.145511	-0.082418	0.961731
445.889672	201.812464	19.150515	-0.082226	0.950616
445.918195	194.358869	19.155520	-0.082226	0.939333
444.145578	187.258224	19.160525	-0.081891	0.927971
442.615981	180.111493	19.165530	-0.081602	0.916461
441.793576	172.831771	19.170535	-0.081444	0.904790
441.474065	165.464760	19.175539	-0.081380	0.892968
440.779087	158.208092	19.180544	-0.081246	0.881059
440.139368	150.956773	19.185549	-0.081122	0.869011
439.721422	143.674507	19.190554	-0.081039	0.856807
438.749741	136.543818	19.195559	-0.080853	0.844518
437.797361	129.407504	19.200563	-0.080671	0.832042
437.254132	122.208361	19.205568	-0.080566	0.819393
436.947267	115.000711	19.210573	-0.080504	0.806604
435.808560	107.993164	19.215578	-0.080287	0.793704
434.358231	101.058433	19.220583	-0.080013	0.780623
433.689673	93.985315	19.225587	-0.079883	0.767318
433.163265	86.942708	19.230592	-0.079781	0.753884
431.985639	80.036425	19.235597	-0.079557	0.740245
430.959896	73.321705	19.240602	-0.079362	0.726781