Mon Apr 19 09:41:11 2021

Number of Points = 3640
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.157991	0.048909	0.000000	-0.000011	0.311445

0.971209	0.087255	0.005005	0.000024	0.311466
0.800984	0.116607	0.010010	0.000056	0.311458
1.143844	0.052899	0.015014	-0.000008	0.311451
0.779868	0.123550	0.020019	0.000060	0.311472
0.840136	0.107927	0.025024	0.000048	0.311450
0.924532	0.054701	0.030029	0.000033	0.311274
0.948731	0.024245	0.035034	0.000028	0.311153
1.003626	0.012938	0.040038	0.000018	0.311146
0.649701	0.080635	0.045043	0.000084	0.311162
1.182231	-0.020687	0.050048	-0.000015	0.311140
1.014394	0.013084	0.055053	0.000016	0.311155
1.071575	-0.000358	0.060058	0.000006	0.311141
1.173224	-0.018270	0.065062	-0.000013	0.311143
1.072891	0.004928	0.070067	0.000006	0.311166
1.012965	0.012380	0.075072	0.000017	0.311150
1.503857	-0.078805	0.080077	-0.000075	0.311141
1.329643	-0.102048	0.085082	-0.000042	0.310885
1.035576	-0.058939	0.090086	0.000013	0.310837
1.097501	-0.068968	0.095091	0.000001	0.310842
0.663089	0.011588	0.100096	0.000082	0.310850
0.346297	0.072586	0.105101	0.000141	0.310866
-0.013609	0.138818	0.110106	0.000208	0.310869
-0.002673	0.136325	0.115110	0.000206	0.310867
0.249670	0.065523	0.120115	0.000159	0.310750
0.084110	0.066366	0.125120	0.000190	0.310614
0.693769	-0.046483	0.130125	0.000077	0.310604
0.564348	-0.024807	0.135130	0.000101	0.310595
0.561849	-0.023217	0.140134	0.000101	0.310600
1.002726	-0.109765	0.145139	0.000019	0.310570
0.933974	-0.168613	0.150144	0.000032	0.310237
0.895700	-0.159243	0.155149	0.000039	0.310249
0.521771	-0.089280	0.160154	0.000109	0.310258
0.863637	-0.154963	0.165158	0.000045	0.310241
0.853207	-0.213467	0.170163	0.000047	0.309959
0.843145	-0.219613	0.175168	0.000049	0.309922
0.771417	-0.202994	0.180173	0.000063	0.309938
0.681306	-0.205340	0.185178	0.000080	0.309850
0.590101	-0.241551	0.190182	0.000097	0.309604
0.564216	-0.235035	0.195187	0.000102	0.309612
1.015882	-0.324047	0.200192	0.000018	0.309579
0.924641	-0.357273	0.205197	0.000035	0.309346
0.830280	-0.348863	0.210202	0.000052	0.309305
1.398213	-0.454626	0.215206	-0.000053	0.309293
1.050009	-0.456989	0.220211	0.000011	0.308986
0.886214	-0.429224	0.225216	0.000042	0.308976
1.528163	-0.566574	0.230221	-0.000077	0.308879
1.049262	-0.525777	0.235226	0.000012	0.308662
0.872375	-0.490868	0.240230	0.000045	0.308675
0.484815	-0.463473	0.245235	0.000117	0.308473
0.486944	-0.489140	0.250240	0.000117	0.308354
0.608029	-0.509816	0.255245	0.000094	0.308360
0.514497	-0.556643	0.260250	0.000112	0.308060
0.466092	-0.547369	0.265254	0.000121	0.308062
0.548896	-0.596285	0.270259	0.000105	0.307903
0.434046	-0.615381	0.275264	0.000127	0.307715
0.785492	-0.684385	0.280269	0.000061	0.307691
1.240136	-0.833018	0.285274	-0.000023	0.307380
0.981356	-0.783866	0.290278	0.000025	0.307390
1.102470	-0.872479	0.295283	0.000003	0.307076
0.883231	-0.834861	0.300288	0.000043	0.307065
1.145766	-0.937565	0.305293	-0.000005	0.306806
0.523422	-0.829473	0.310298	0.000111	0.306782
0.436357	-0.873170	0.315302	0.000127	0.306501
0.845791	-0.958525	0.320307	0.000051	0.306449
0.980971	-1.041121	0.325312	0.000026	0.306175
1.107098	-1.076531	0.330317	0.000002	0.306116
0.863445	-1.093779	0.335322	0.000048	0.305824
0.532653	-1.037288	0.340326	0.000109	0.305807
0.552625	-1.089617	0.345331	0.000106	0.305576
0.549189	-1.104571	0.350336	0.000106	0.305502
0.619849	-1.172316	0.355341	0.000093	0.305242
0.622661	-1.202208	0.360346	0.000093	0.305103
0.298166	-1.182099	0.365350	0.000153	0.304918
0.189888	-1.199828	0.370355	0.000173	0.304740
-0.154206	-1.171395	0.375360	0.000237	0.304578
-0.446594	-1.159141	0.380365	0.000292	0.304384
0.158592	-1.288782	0.385370	0.000179	0.304290
0.368617	-1.389030	0.390374	0.000140	0.303995
0.532162	-1.441268	0.395379	0.000110	0.303887
0.277582	-1.446885	0.400384	0.000157	0.303640
0.393691	-1.503608	0.405389	0.000136	0.303470
0.330998	-1.519666	0.410394	0.000148	0.303339
0.204860	-1.558245	0.415398	0.000171	0.303045
0.600090	-1.659083	0.420403	0.000098	0.302906
0.250952	-1.637895	0.425408	0.000163	0.302704
-0.023698	-1.642966	0.430413	0.000214	0.302441
-0.349574	-1.613680	0.435418	0.000275	0.302298
-0.305572	-1.671596	0.440422	0.000267	0.302058
-0.727866	-1.634603	0.445427	0.000345	0.301868
-1.056134	-1.597365	0.450432	0.000406	0.301760
-0.293400	-1.803040	0.455437	0.000265	0.301438
0.288395	-1.943316	0.460442	0.000156	0.301272
-0.080363	-1.909840	0.465446	0.000225	0.301111
-0.195722	-1.946220	0.470451	0.000247	0.300835
0.199326	-2.051262	0.475456	0.000173	0.300675
0.315733	-2.110833	0.480461	0.000152	0.300490
-0.559140	-2.001671	0.485466	0.000314	0.300249
-0.526001	-2.064007	0.490470	0.000308	0.299978
-0.441241	-2.116398	0.495475	0.000293	0.299799
-1.278186	-2.005102	0.500480	0.000448	0.299602
-1.958373	-1.937177	0.505485	0.000575	0.299333
-2.057025	-1.947165	0.510490	0.000593	0.299197
-1.280579	-2.137182	0.515494	0.000449	0.298961
-0.569796	-2.320441	0.520499	0.000317	0.298699
-0.440750	-2.392704	0.525504	0.000293	0.298462
-1.526913	-2.231172	0.530509	0.000495	0.298288
-1.928252	-2.209773	0.535514	0.000570	0.298037
-1.520537	-2.331609	0.540518	0.000494	0.297805
-1.668031	-2.344696	0.545523	0.000522	0.297611
-2.374069	-2.261977	0.550528	0.000653	0.297389
-2.000770	-2.388190	0.555533	0.000584	0.297105
-3.146360	-2.208990	0.560538	0.000797	0.296963
-3.108038	-2.253104	0.565542	0.000790	0.296782
-2.556023	-2.412312	0.570547	0.000687	0.296495
-3.645107	-2.248980	0.575552	0.000890	0.296325
-4.211341	-2.182028	0.580557	0.000995	0.296150
-4.089022	-2.252049	0.585562	0.000973	0.295916
-4.590417	-2.180884	0.590566	0.001066	0.295818
-5.027388	-2.143855	0.595571	0.001147	0.295610
-4.885791	-2.201474	0.600576	0.001121	0.295454
-4.710126	-2.277094	0.605581	0.001089	0.295240
-5.033210	-2.265312	0.610586	0.001149	0.295009
-5.635116	-2.174831	0.615590	0.001261	0.294916
-5.770850	-2.213466	0.620595	0.001286	0.294605
-5.465366	-2.292796	0.625600	0.001229	0.294488
-5.674397	-2.293631	0.630605	0.001268	0.294297
-5.882087	-2.295814	0.635610	0.001307	0.294100
-6.216767	-2.264349	0.640614	0.001369	0.293956
-6.236394	-2.316678	0.645619	0.001373	0.293680
-6.655137	-2.257310	0.650624	0.001451	0.293598
-6.642884	-2.314407	0.655629	0.001449	0.293327
-6.532862	-2.358952	0.660634	0.001428	0.293205
-7.033691	-2.303485	0.665638	0.001522	0.293030
-7.152448	-2.319547	0.670643	0.001544	0.292843
-7.870455	-2.217249	0.675648	0.001678	0.292704
-8.227806	-2.197916	0.680653	0.001744	0.292478
-8.555693	-2.153737	0.685658	0.001805	0.292401
-8.465182	-2.219283	0.690662	0.001788	0.292158
-8.840362	-2.164025	0.695667	0.001858	0.292094
-9.067878	-2.170005	0.700672	0.001901	0.291859
-9.276380	-2.142462	0.705677	0.001940	0.291807
-9.200626	-2.203951	0.710682	0.001926	0.291570
-9.701938	-2.135543	0.715686	0.002019	0.291457
-9.306036	-2.243221	0.720691	0.001945	0.291280
-9.684888	-2.203979	0.725696	0.002016	0.291132
-9.891322	-2.198264	0.730701	0.002054	0.290974
-9.942986	-2.219737	0.735706	0.002064	0.290820
-9.988276	-2.237747	0.740710	0.002073	0.290689
-10.532293	-2.161477	0.745715	0.002174	0.290577
-10.890517	-2.117546	0.750720	0.002241	0.290471
-10.665989	-2.205237	0.755725	0.002199	0.290237
-11.018472	-2.149215	0.760730	0.002264	0.290197
-11.614994	-2.094473	0.765734	0.002376	0.289928
-11.513524	-2.109712	0.770739	0.002357	0.289944
-11.482222	-2.176937	0.775744	0.002351	0.289637
-11.809743	-2.124750	0.780749	0.002412	0.289600
-11.953530	-2.132517	0.785754	0.002439	0.289430
-11.993337	-2.148857	0.790758	0.002446	0.289312
-11.670835	-2.232411	0.795763	0.002386	0.289187
-12.605775	-2.106534	0.800768	0.002560	0.288966
-12.407370	-2.144600	0.805773	0.002523	0.288956
-12.660495	-2.157996	0.810778	0.002571	0.288658
-13.074007	-2.083049	0.815782	0.002648	0.288657
-12.621926	-2.210371	0.820787	0.002564	0.288430
-12.995298	-2.162775	0.825792	0.002633	0.288328
-13.227119	-2.143888	0.830797	0.002676	0.288211
-13.646042	-2.096698	0.835802	0.002754	0.288065
-13.517969	-2.122885	0.840806	0.002731	0.288050
-13.862606	-2.122885	0.845811	0.002795	0.287735
-14.320836	-2.043010	0.850816	0.002880	0.287718
-13.759609	-2.180675	0.855821	0.002776	0.287538
-13.811071	-2.200150	0.860826	0.002785	0.287393
-14.058496	-2.174658	0.865830	0.002831	0.287295
-14.878798	-2.067448	0.870835	0.002984	0.287083
-14.662666	-2.110269	0.875840	0.002944	0.287065
-14.615834	-2.159007	0.880845	0.002935	0.286862
-14.581061	-2.181162	0.885850	0.002929	0.286782
-14.683895	-2.188152	0.890854	0.002948	0.286652
-15.335406	-2.107771	0.895859	0.003069	0.286459
-15.650324	-2.050637	0.900864	0.003128	0.286459
-15.152458	-2.193639	0.905869	0.003036	0.286193
-15.603153	-2.118449	0.910874	0.003119	0.286159
-16.183304	-2.038670	0.915878	0.003227	0.286029
-16.393283	-2.036239	0.920883	0.003267	0.285847
-16.260117	-2.061666	0.925888	0.003242	0.285841
-16.282921	-2.093272	0.930893	0.003246	0.285660
-16.643729	-2.042645	0.935898	0.003313	0.285584
-16.127288	-2.152146	0.940902	0.003217	0.285504
-16.303842	-2.171242	0.945907	0.003250	0.285244
-16.784928	-2.086517	0.950912	0.003340	0.285230
-16.865479	-2.112601	0.955917	0.003355	0.285023
-16.904185	-2.125386	0.960922	0.003362	0.284922
-17.256264	-2.072588	0.965926	0.003428	0.284865
-17.539496	-2.073004	0.970931	0.003480	0.284601
-17.424799	-2.097052	0.975936	0.003459	0.284585
-17.349071	-2.139670	0.980941	0.003445	0.284438
-18.122147	-2.024159	0.985946	0.003589	0.284310
-17.846970	-2.072786	0.990950	0.003538	0.284317
-17.665271	-2.166035	0.995955	0.003504	0.284010
-18.488872	-2.023804	1.000960	0.003658	0.283971
-18.235978	-2.090814	1.005965	0.003610	0.283864
-18.119253	-2.151317	1.010970	0.003589	0.283663
-18.315222	-2.117234	1.015974	0.003625	0.283655
-18.500128	-2.130219	1.020979	0.003660	0.283417
-18.708027	-2.108275	1.025984	0.003699	0.283336
-18.689903	-2.124619	1.030989	0.003695	0.283269
-19.356170	-2.046154	1.035994	0.003819	0.283051
-19.153677	-2.084652	1.040998	0.003782	0.283042
-19.039148	-2.140936	1.046003	0.003760	0.282860
-19.754147	-2.040690	1.051008	0.003894	0.282708
-19.450577	-2.095206	1.056013	0.003837	0.282711
-19.310496	-2.178396	1.061018	0.003811	0.282415
-19.863883	-2.082357	1.066022	0.003914	0.282391
-19.954233	-2.087496	1.071027	0.003931	0.282281
-20.107686	-2.101084	1.076032	0.003960	0.282068
-19.341026	-2.242274	1.081037	0.003817	0.282058
-19.810478	-2.206675	1.086042	0.003904	0.281802
-20.340736	-2.118821	1.091046	0.004003	0.281758
-19.863405	-2.231408	1.096051	0.003914	0.281625
-20.309993	-2.189965	1.101056	0.003998	0.281421
-20.353914	-2.182107	1.106061	0.004006	0.281420
-20.257187	-2.257021	1.111066	0.003988	0.281125
-20.353685	-2.242187	1.116070	0.004006	0.281111
-20.517850	-2.251068	1.121075	0.004037	0.280911
-21.200784	-2.148476	1.126080	0.004164	0.280799
-20.857934	-2.218702	1.131085	0.004100	0.280758
-21.574080	-2.121997	1.136090	0.004233	0.280585
-21.848701	-2.071797	1.141094	0.004284	0.280587
-21.047238	-2.257299	1.146099	0.004135	0.280381
-21.983375	-2.114616	1.151104	0.004310	0.280239
-21.664963	-2.180731	1.156109	0.004250	0.280196
-21.684353	-2.233277	1.161114	0.004254	0.279906
-21.513232	-2.268023	1.166118	0.004222	0.279887
-21.694488	-2.279711	1.171123	0.004256	0.279656
-22.299374	-2.183937	1.176128	0.004369	0.279582
-21.722297	-2.310337	1.181133	0.004261	0.279470
-22.734170	-2.157531	1.186138	0.004450	0.279309
-23.088222	-2.094663	1.191142	0.004516	0.279301
-22.936078	-2.169937	1.196147	0.004487	0.279054
-23.285524	-2.122579	1.201152	0.004552	0.278969
-23.333070	-2.124831	1.206157	0.004561	0.278913
-23.218143	-2.195641	1.211162	0.004540	0.278653
-23.395103	-2.164122	1.216166	0.004573	0.278649
-23.479911	-2.184589	1.221171	0.004589	0.278463
-24.030307	-2.110516	1.226176	0.004691	0.278327
-23.864262	-2.137650	1.231181	0.004661	0.278343
-23.525316	-2.260100	1.236186	0.004598	0.278026
-24.031743	-2.167732	1.241190	0.004692	0.278027
-23.744708	-2.250971	1.246195	0.004638	0.277866
-24.459845	-2.152756	1.251200	0.004772	0.277699
-24.376936	-2.168107	1.256205	0.004756	0.277698
-24.789215	-2.150035	1.261210	0.004833	0.277401
-25.009623	-2.111313	1.266214	0.004874	0.277394
-25.497345	-2.033848	1.271219	0.004965	0.277335
-25.515322	-2.080396	1.276224	0.004968	0.277074
-25.233297	-2.130133	1.281229	0.004916	0.277082
-25.650596	-2.077235	1.286234	0.004994	0.276962
-26.107578	-2.026618	1.291238	0.005079	0.276792
-25.630990	-2.112364	1.296243	0.004990	0.276796
-26.060022	-2.077411	1.301248	0.005070	0.276571
-26.254053	-2.063864	1.306253	0.005106	0.276457
-25.846230	-2.137785	1.311258	0.005030	0.276458
-26.067787	-2.156437	1.316262	0.005072	0.276149
-26.566129	-2.063001	1.321267	0.005164	0.276163
-27.070351	-1.981142	1.326272	0.005258	0.276111
-26.640471	-2.110848	1.331277	0.005178	0.275841
-26.624986	-2.112610	1.336282	0.005175	0.275846
-26.765853	-2.114113	1.341286	0.005202	0.275704
-26.760255	-2.137363	1.346291	0.005201	0.275587
-26.930824	-2.105258	1.351296	0.005233	0.275592
-27.281132	-2.095982	1.356301	0.005298	0.275306
-27.354806	-2.092328	1.361306	0.005312	0.275254
-27.412595	-2.092674	1.366310	0.005322	0.275197
-27.462067	-2.132489	1.371315	0.005332	0.274940
-27.485476	-2.131445	1.376320	0.005336	0.274923
-27.564585	-2.148590	1.381325	0.005351	0.274756
-27.937157	-2.108820	1.386330	0.005420	0.274609
-28.327134	-2.036587	1.391334	0.005493	0.274615
-27.981006	-2.144883	1.396339	0.005429	0.274376
-28.288402	-2.098155	1.401344	0.005486	0.274327
-28.374245	-2.099811	1.406349	0.005502	0.274236
-28.663281	-2.094546	1.411354	0.005556	0.273986
-28.383038	-2.147853	1.416358	0.005504	0.273973
-28.511865	-2.155780	1.421363	0.005528	0.273807
-29.275702	-2.041340	1.426368	0.005670	0.273678
-28.868248	-2.116713	1.431373	0.005594	0.273671
-28.596634	-2.223432	1.436378	0.005544	0.273367
-29.260971	-2.106770	1.441382	0.005667	0.273345
-29.480787	-2.084018	1.446387	0.005708	0.273253
-29.109868	-2.190614	1.451392	0.005639	0.273046
-29.617149	-2.095584	1.456397	0.005734	0.273060
-29.376452	-2.190464	1.461402	0.005689	0.272789
-29.453094	-2.191788	1.466406	0.005703	0.272707
-29.527002	-2.195949	1.471411	0.005717	0.272614
-30.148698	-2.123470	1.476416	0.005833	0.272398
-29.902757	-2.168878	1.481421	0.005787	0.272394
-29.853936	-2.226200	1.486426	0.005778	0.272136
-30.672652	-2.089142	1.491430	0.005931	0.272073
-29.640277	-2.293555	1.496435	0.005738	0.271984
-29.797637	-2.307761	1.501440	0.005768	0.271756
-30.282428	-2.216146	1.506445	0.005858	0.271774
-30.740683	-2.192981	1.511450	0.005943	0.271453
-30.984113	-2.148746	1.516454	0.005989	0.271452
-30.616879	-2.243108	1.521459	0.005920	0.271305
-31.440312	-2.124658	1.526464	0.006074	0.271138
-31.349647	-2.138576	1.531469	0.006057	0.271151
-31.588160	-2.144274	1.536474	0.006101	0.270889
-31.873116	-2.103464	1.541478	0.006154	0.270830
-31.617536	-2.161488	1.546483	0.006107	0.270768
-31.809013	-2.162644	1.551488	0.006143	0.270575
-31.905429	-2.145181	1.556493	0.006161	0.270574
-31.426083	-2.281466	1.561498	0.006072	0.270311
-31.227969	-2.339380	1.566502	0.006035	0.270194
-31.020635	-2.406248	1.571507	0.005996	0.270037
-32.186751	-2.223466	1.576512	0.006213	0.269880
-32.218363	-2.221422	1.581517	0.006219	0.269860
-31.587956	-2.391971	1.586522	0.006102	0.269559
-32.615799	-2.203152	1.591526	0.006293	0.269569
-33.310417	-2.115688	1.596531	0.006423	0.269360
-32.816395	-2.219848	1.601536	0.006331	0.269283
-32.653040	-2.270040	1.606541	0.006300	0.269173
-33.606406	-2.135920	1.611546	0.006478	0.268961
-33.627968	-2.133125	1.616550	0.006482	0.268955
-33.280110	-2.234353	1.621555	0.006417	0.268750
-33.660259	-2.185505	1.626560	0.006488	0.268640
-33.927331	-2.145518	1.631565	0.006538	0.268594
-33.697631	-2.236570	1.636570	0.006495	0.268328
-34.494430	-2.090769	1.641574	0.006643	0.268332
-34.484789	-2.120216	1.646579	0.006642	0.268183
-34.459474	-2.149649	1.651584	0.006637	0.268048
-34.181500	-2.202080	1.656589	0.006585	0.268038
-34.284514	-2.247669	1.661594	0.006605	0.267690
-34.479841	-2.213566	1.666598	0.006641	0.267682
-34.432718	-2.249738	1.671603	0.006632	0.267533
-35.065404	-2.162382	1.676608	0.006750	0.267382
-34.949996	-2.185380	1.681613	0.006729	0.267371
-34.514314	-2.322185	1.686618	0.006648	0.267059
-35.069517	-2.221933	1.691622	0.006751	0.267055
-35.707617	-2.131389	1.696627	0.006870	0.266916
-35.549197	-2.186338	1.701632	0.006840	0.266774
-35.356943	-2.226132	1.706637	0.006805	0.266748
-36.074323	-2.151309	1.711642	0.006938	0.266445
-36.083538	-2.150616	1.716646	0.006940	0.266439
-35.724150	-2.241306	1.721651	0.006873	0.266302
-36.099712	-2.204377	1.726656	0.006943	0.266131
-36.299517	-2.168905	1.731661	0.006980	0.266126
-36.202144	-2.241476	1.736666	0.006962	0.265827
-36.307482	-2.227197	1.741670	0.006982	0.265800
-36.551393	-2.204587	1.746675	0.007027	0.265681
-36.783691	-2.186090	1.751680	0.007071	0.265551
-36.645626	-2.211540	1.756685	0.007045	0.265549
-36.717028	-2.263423	1.761690	0.007058	0.265195
-37.105863	-2.193802	1.766694	0.007131	0.265189
-36.958118	-2.249061	1.771699	0.007103	0.265034
-37.346291	-2.205682	1.776704	0.007176	0.264884
-37.201267	-2.239506	1.781709	0.007149	0.264844
-37.884167	-2.163701	1.786714	0.007276	0.264578
-37.929127	-2.157946	1.791718	0.007284	0.264565
-38.017688	-2.167425	1.796723	0.007301	0.264425
-38.256457	-2.150499	1.801728	0.007345	0.264279
-38.195078	-2.159936	1.806733	0.007334	0.264288
-38.043110	-2.244932	1.811738	0.007306	0.263974
-38.405552	-2.187615	1.816742	0.007373	0.263926
-38.107947	-2.263406	1.821747	0.007318	0.263807
-38.526356	-2.218923	1.826752	0.007396	0.263633
-38.765149	-2.178387	1.831757	0.007440	0.263617
-38.389364	-2.303840	1.836762	0.007371	0.263303
-38.582402	-2.270835	1.841766	0.007407	0.263291
-38.656358	-2.287420	1.846771	0.007420	0.263126
-39.519304	-2.148533	1.851776	0.007581	0.263026
-39.051428	-2.243076	1.856781	0.007494	0.262974
-39.139907	-2.279803	1.861786	0.007511	0.262682
-39.842401	-2.154025	1.866790	0.007641	0.262671
-39.939860	-2.167875	1.871795	0.007659	0.262497
-39.933347	-2.192201	1.876800	0.007658	0.262369
-39.969920	-2.189594	1.881805	0.007665	0.262346
-40.135407	-2.215397	1.886810	0.007696	0.262037
-39.990511	-2.244653	1.891814	0.007669	0.262021
-40.309695	-2.214861	1.896819	0.007729	0.261864
-40.669303	-2.170092	1.901824	0.007796	0.261750
-40.043526	-2.292174	1.906829	0.007679	0.261704
-40.313174	-2.294590	1.911834	0.007729	0.261419
-40.774651	-2.213477	1.916838	0.007815	0.261403
-40.848248	-2.235601	1.921843	0.007829	0.261206
-40.776867	-2.267729	1.926848	0.007816	0.261099
-40.845567	-2.274009	1.931853	0.007829	0.260995
-41.344036	-2.220920	1.936858	0.007922	0.260786
-41.327340	-2.224311	1.941862	0.007918	0.260784
-41.037200	-2.315132	1.946867	0.007865	0.260572
-41.710743	-2.199249	1.951872	0.007990	0.260535
-41.671260	-2.233048	1.956877	0.007983	0.260387
-42.213372	-2.163948	1.961882	0.008084	0.260222
-42.319087	-2.147057	1.966886	0.008103	0.260209
-42.214563	-2.213329	1.971891	0.008084	0.259946
-42.327472	-2.201261	1.976896	0.008105	0.259898
-42.608129	-2.172361	1.981901	0.008157	0.259774
-42.869970	-2.159840	1.986906	0.008206	0.259578
-42.847019	-2.166846	1.991910	0.008202	0.259562
-43.090599	-2.158320	1.996915	0.008247	0.259362
-43.137154	-2.165855	2.001920	0.008256	0.259273

-42.842000	-2.280684	2.011917	0.008201	0.258930
-43.435688	-2.206260	2.021914	0.008312	0.258742
-43.947899	-2.129780	2.031910	0.008407	0.258648
-44.145796	-2.142703	2.041907	0.008444	0.258373
-44.589444	-2.070017	2.051904	0.008527	0.258328
-44.361750	-2.134912	2.061901	0.008485	0.258196
-44.090792	-2.216817	2.071898	0.008434	0.258012
-44.155242	-2.205036	2.081894	0.008446	0.258012
-44.407775	-2.194914	2.091891	0.008493	0.257811
-44.931575	-2.120417	2.101888	0.008591	0.257693
-44.430583	-2.215426	2.111885	0.008498	0.257671
-44.510476	-2.200276	2.121882	0.008513	0.257674
-44.756258	-2.153471	2.131878	0.008559	0.257685
-44.665719	-2.169262	2.141875	0.008542	0.257689
-44.682954	-2.167823	2.151872	0.008545	0.257679
-44.254787	-2.246638	2.161869	0.008466	0.257673
-44.956243	-2.126806	2.171866	0.008596	0.257629
-45.185266	-2.071609	2.181862	0.008639	0.257704
-44.612192	-2.178950	2.191859	0.008532	0.257686
-44.894287	-2.126119	2.201856	0.008585	0.257694
-44.747010	-2.152751	2.211853	0.008558	0.257695
-45.063215	-2.093558	2.221850	0.008617	0.257704
-44.597468	-2.178898	2.231846	0.008530	0.257700
-44.577751	-2.122534	2.241843	0.008526	0.258036
-44.700001	-2.100126	2.251840	0.008549	0.258036
-44.897791	-2.060957	2.261837	0.008586	0.258054
-44.940455	-2.019366	2.271834	0.008594	0.258243
-44.683557	-2.048983	2.281830	0.008546	0.258339
-44.859763	-2.006663	2.291827	0.008579	0.258396
-44.675795	-1.989867	2.301824	0.008545	0.258677
-44.586288	-2.006626	2.311821	0.008528	0.258674
-44.264062	-2.013074	2.321818	0.008469	0.258965
-44.024521	-2.054481	2.331814	0.008424	0.258977
-43.897391	-2.032047	2.341811	0.008400	0.259231
-43.695486	-2.056636	2.351808	0.008363	0.259298
-43.058836	-2.140797	2.361805	0.008245	0.259475
-42.815621	-2.169431	2.371802	0.008199	0.259561
-42.568485	-2.192334	2.381798	0.008153	0.259684
-42.359764	-2.193221	2.391795	0.008115	0.259890
-43.014318	-2.058319	2.401792	0.008237	0.259978
-42.400434	-2.126477	2.411789	0.008122	0.260220
-42.149535	-2.152818	2.421786	0.008076	0.260327
-41.714226	-2.190159	2.431782	0.007995	0.260559
-41.738130	-2.172295	2.441779	0.007999	0.260634
-41.630806	-2.162741	2.451776	0.007979	0.260795
-41.577912	-2.145752	2.461773	0.007970	0.260942
-41.747523	-2.080307	2.471770	0.008001	0.261133
-41.237515	-2.130126	2.481766	0.007906	0.261371
-41.586146	-2.042278	2.491763	0.007971	0.261506
-41.369446	-2.031174	2.501760	0.007931	0.261785
-40.938614	-2.075125	2.511757	0.007851	0.261975
-40.798078	-2.077322	2.521754	0.007825	0.262103
-40.375662	-2.103650	2.531750	0.007746	0.262382
-40.599697	-2.027268	2.541747	0.007788	0.262578
-40.595255	-1.990989	2.551744	0.007787	0.262782
-40.505591	-1.957358	2.561741	0.007771	0.263057
-40.087730	-1.988235	2.571738	0.007693	0.263305
-39.543352	-2.052898	2.581734	0.007592	0.263493
-39.304169	-2.067037	2.591731	0.007547	0.263654
-38.991336	-2.069244	2.601728	0.007489	0.263954
-39.104824	-2.009408	2.611725	0.007510	0.264168
-38.634133	-2.062313	2.621722	0.007423	0.264347
-38.496379	-2.045640	2.631718	0.007397	0.264575
-38.189474	-2.051489	2.641715	0.007340	0.264848
-37.741409	-2.102549	2.651712	0.007257	0.265014
-37.102471	-2.186112	2.661709	0.007138	0.265192
-37.176864	-2.115793	2.671706	0.007152	0.265501
-37.083097	-2.101998	2.681702	0.007135	0.265669
-36.620384	-2.161622	2.691699	0.007049	0.265802
-36.088269	-2.205762	2.701696	0.006950	0.266089
-35.955208	-2.204835	2.711693	0.006925	0.266225
-35.273594	-2.293225	2.721690	0.006798	0.266418
-35.392876	-2.224974	2.731686	0.006821	0.266670
-35.681498	-2.141549	2.741683	0.006874	0.266838
-35.567512	-2.120361	2.751680	0.006853	0.267065
-35.430813	-2.092578	2.761677	0.006828	0.267349
-34.755783	-2.184833	2.771674	0.006702	0.267514
-34.123039	-2.269307	2.781670	0.006585	0.267679
-34.741406	-2.093101	2.791667	0.006700	0.268024
-33.898211	-2.213323	2.801664	0.006543	0.268202
-33.785916	-2.205387	2.811661	0.006522	0.268355
-33.208444	-2.259673	2.821658	0.006415	0.268628
-32.687919	-2.322170	2.831654	0.006318	0.268801
-33.190582	-2.198926	2.841651	0.006411	0.268972
-33.037982	-2.168682	2.851648	0.006383	0.269283
-32.345329	-2.261340	2.861645	0.006254	0.269462
-32.277077	-2.242253	2.871642	0.006242	0.269631
-32.276635	-2.193399	2.881638	0.006242	0.269893
-32.201247	-2.157774	2.891635	0.006228	0.270157
-32.113258	-2.126899	2.901632	0.006211	0.270408
-31.565026	-2.193115	2.911629	0.006109	0.270586
-31.534300	-2.154941	2.921626	0.006104	0.270820
-30.716099	-2.257773	2.931622	0.005951	0.271065
-30.658614	-2.239061	2.941619	0.005941	0.271221
-30.331822	-2.260948	2.951616	0.005880	0.271420
-30.482604	-2.173334	2.961613	0.005908	0.271741
-29.935662	-2.236162	2.971610	0.005807	0.271936
-29.669856	-2.251528	2.981606	0.005757	0.272111
-29.540252	-2.225756	2.991603	0.005733	0.272373
-29.551060	-2.173965	3.001600	0.005735	0.272637
-29.667870	-2.105651	3.011597	0.005757	0.272886
-28.766778	-2.230260	3.021594	0.005589	0.273094
-28.367958	-2.262239	3.031590	0.005515	0.273309
-28.572401	-2.171598	3.041587	0.005553	0.273591
-28.182528	-2.204694	3.051584	0.005481	0.273791
-27.886728	-2.219319	3.061581	0.005426	0.273997
-27.661314	-2.204389	3.071578	0.005384	0.274292
-27.706443	-2.149906	3.081574	0.005392	0.274536
-27.186269	-2.203785	3.091571	0.005296	0.274750
-27.311777	-2.136652	3.101568	0.005319	0.274983
-27.347665	-2.080512	3.111565	0.005326	0.275244
-26.633554	-2.147016	3.121562	0.005193	0.275576
-26.308552	-2.174642	3.131558	0.005133	0.275741
-26.124671	-2.168356	3.141555	0.005098	0.275949
-25.916645	-2.165637	3.151552	0.005060	0.276161
-25.584746	-2.173901	3.161549	0.004998	0.276434
-25.083603	-2.214790	3.171546	0.004905	0.276696
-25.270626	-2.138205	3.181542	0.004940	0.276919
-24.700487	-2.205035	3.191539	0.004834	0.277111
-24.815291	-2.132669	3.201536	0.004855	0.277379
-24.113994	-2.205089	3.211533	0.004725	0.277666
-24.163471	-2.150474	3.221530	0.004734	0.277903
-23.780133	-2.178972	3.231526	0.004663	0.278117
-23.981991	-2.096078	3.241523	0.004700	0.278357
-23.267738	-2.171280	3.251520	0.004567	0.278641
-23.404568	-2.097911	3.261517	0.004593	0.278892
-22.980346	-2.128702	3.271514	0.004514	0.279132
-22.477217	-2.180479	3.281510	0.004420	0.279338
-22.109373	-2.202079	3.291507	0.004352	0.279572
-21.958702	-2.177206	3.301504	0.004324	0.279842
-22.007767	-2.120490	3.311501	0.004333	0.280089
-21.666830	-2.136480	3.321498	0.004270	0.280326
-21.855799	-2.049046	3.331494	0.004305	0.280599
-21.488599	-2.072078	3.341491	0.004237	0.280825
-21.430096	-2.031444	3.351488	0.004226	0.281088
-20.880656	-2.082962	3.361485	0.004124	0.281337
-20.527533	-2.101219	3.371482	0.004058	0.281573
-19.864923	-2.180680	3.381478	0.003935	0.281783
-19.956658	-2.109709	3.391475	0.003952	0.282061
-19.958642	-2.058726	3.401472	0.003952	0.282321
-19.346182	-2.122703	3.411469	0.003839	0.282563
-19.223986	-2.101365	3.421466	0.003816	0.282786
-18.882403	-2.113020	3.431462	0.003752	0.283043
-18.361045	-2.154833	3.441459	0.003655	0.283314
-18.258022	-2.134044	3.451456	0.003636	0.283515
-17.999395	-2.137057	3.461453	0.003588	0.283739
-17.974805	-2.095778	3.471450	0.003584	0.283972
-17.143019	-2.186298	3.481446	0.003429	0.284281
-16.927551	-2.188912	3.491443	0.003389	0.284466
-16.767927	-2.184942	3.501440	0.003359	0.284634
-16.191407	-2.240152	3.511437	0.003252	0.284886
-16.649826	-2.101619	3.521434	0.003337	0.285165
-15.882170	-2.199363	3.531430	0.003195	0.285377
-15.849337	-2.163866	3.541427	0.003189	0.285587
-15.560236	-2.174894	3.551424	0.003135	0.285797
-15.357066	-2.160824	3.561421	0.003097	0.286055
-15.169423	-2.154157	3.571418	0.003062	0.286260
-14.966060	-2.148512	3.581414	0.003025	0.286475
-14.683606	-2.141472	3.591411	0.002972	0.286770
-14.336933	-2.159713	3.601408	0.002908	0.286995
-14.140976	-2.156232	3.611405	0.002871	0.287192
-13.916693	-2.153513	3.621402	0.002829	0.287411
-13.322325	-2.206667	3.631398	0.002719	0.287687
-13.132540	-2.196434	3.641395	0.002684	0.287911
-13.146278	-2.154429	3.651392	0.002686	0.288109
-12.422858	-2.246984	3.661389	0.002552	0.288304
-12.175065	-2.234847	3.671386	0.002506	0.288591
-12.433110	-2.149661	3.681382	0.002554	0.288782
-11.831414	-2.223270	3.691379	0.002442	0.288961
-11.084785	-2.298544	3.701376	0.002303	0.289263
-11.544219	-2.178539	3.711373	0.002389	0.289445
-10.916780	-2.259606	3.721370	0.002272	0.289610
-10.298171	-2.319081	3.731366	0.002157	0.289874
-10.302578	-2.278834	3.741363	0.002158	0.290070
-10.163769	-2.269211	3.751360	0.002132	0.290244
-9.962584	-2.247168	3.761357	0.002095	0.290536
-9.802182	-2.238863	3.771354	0.002065	0.290722
-9.621087	-2.237767	3.781350	0.002031	0.290891
-9.338743	-2.244414	3.791347	0.001979	0.291112
-9.151750	-2.222502	3.801344	0.001944	0.291390
-9.085626	-2.193279	3.811341	0.001932	0.291594
-8.656639	-2.228967	3.821338	0.001852	0.291803
-8.918051	-2.129052	3.831334	0.001901	0.292063
-8.572958	-2.138178	3.841331	0.001836	0.292328
-8.595843	-2.086224	3.851328	0.001841	0.292564
-8.150898	-2.119689	3.861325	0.001758	0.292798
-7.713074	-2.147025	3.871322	0.001677	0.293055
-8.123043	-2.014454	3.881318	0.001753	0.293342
-7.640862	-2.050888	3.891315	0.001663	0.293594
-7.539499	-2.020513	3.901312	0.001644	0.293834
-8.069979	-1.864964	3.911309	0.001743	0.294124
-6.743899	-2.054912	3.921306	0.001496	0.294375
-6.231682	-2.104641	3.931302	0.001401	0.294588
-5.608602	-2.156287	3.941299	0.001285	0.294890
-5.836862	-2.075337	3.951296	0.001328	0.295083
-6.272230	-1.943134	3.961293	0.001409	0.295343
-6.184256	-1.902254	3.971290	0.001393	0.295621
-5.527788	-1.983327	3.981286	0.001271	0.295807
-4.670214	-2.075490	3.991283	0.001111	0.296118
-3.774573	-2.199562	4.001280	0.000944	0.296307
-4.289921	-2.062905	4.011277	0.001040	0.296517
-4.363391	-1.998645	4.021274	0.001054	0.296764
-4.864380	-1.850553	4.031270	0.001147	0.297042
-4.969620	-1.766930	4.041267	0.001167	0.297356
-4.190389	-1.848011	4.051264	0.001022	0.297650
-3.721994	-1.870148	4.061261	0.000935	0.297955
-3.147695	-1.926474	4.071258	0.000828	0.298188
-4.634120	-1.595988	4.081254	0.001105	0.298480
-4.401205	-1.570044	4.091251	0.001061	0.298811
-4.610281	-1.458959	4.101248	0.001100	0.299164
-3.617060	-1.572348	4.111245	0.000916	0.299488
-3.500223	-1.529128	4.121242	0.000894	0.299799
-2.257304	-1.691027	4.131238	0.000663	0.300107
-3.442454	-1.409987	4.141235	0.000883	0.300423
-3.688683	-1.300978	4.151232	0.000929	0.300732
-3.858037	-1.198533	4.161229	0.000961	0.301076
-3.552876	-1.166234	4.171226	0.000904	0.301497
-2.256680	-1.329182	4.181222	0.000663	0.301845
-2.099831	-1.292923	4.191219	0.000634	0.302155
-2.124497	-1.219307	4.201216	0.000638	0.302485
-2.287793	-1.112723	4.211213	0.000669	0.302853
-2.941554	-0.916560	4.221210	0.000790	0.303222
-2.809192	-0.852461	4.231206	0.000766	0.303642
-2.256668	-0.865903	4.241203	0.000663	0.304055
-1.326897	-0.961107	4.251200	0.000490	0.304406
-0.759421	-0.990422	4.261197	0.000385	0.304756
-1.102847	-0.851119	4.271194	0.000448	0.305120
-1.589025	-0.670279	4.281190	0.000539	0.305558
-1.580193	-0.592058	4.291187	0.000537	0.305935
-1.241110	-0.572042	4.301184	0.000474	0.306321
-1.304543	-0.466760	4.311181	0.000486	0.306763
-1.046176	-0.424323	4.321178	0.000438	0.307184
-0.717251	-0.397856	4.331174	0.000377	0.307589
-0.964215	-0.249609	4.341171	0.000423	0.308075
-1.035646	-0.146025	4.351168	0.000436	0.308500
-0.817607	-0.090479	4.361165	0.000396	0.308945
-0.979251	0.041984	4.371162	0.000426	0.309427
-0.500502	0.053813	4.381158	0.000337	0.309888
-0.225196	0.108625	4.391155	0.000285	0.310377
0.000000	0.155246	4.401152	0.000244	0.310784

-0.367736	0.506883	4.406157	0.000312	0.312107
0.025275	1.000643	4.411162	0.000238	0.314716
-0.113358	1.874732	4.416166	0.000264	0.318595
-0.222963	3.033057	4.421171	0.000283	0.323723
0.706654	4.286968	4.426176	0.000110	0.330020
0.788851	5.999880	4.431181	0.000093	0.337510
1.675915	7.864089	4.436186	-0.000073	0.346082
2.557096	10.046680	4.441190	-0.000239	0.355740
4.735734	12.303097	4.446195	-0.000646	0.366364
7.166043	14.854059	4.451200	-0.001100	0.377992
7.721423	18.093516	4.456205	-0.001205	0.390565
8.049177	21.700254	4.461210	-0.001269	0.403915
8.674422	25.596525	4.466214	-0.001388	0.418027
10.258775	29.672383	4.471219	-0.001685	0.432860
11.166793	34.215473	4.476224	-0.001857	0.448314
11.950520	39.144059	4.481229	-0.002006	0.464384
14.009242	44.188674	4.486234	-0.002393	0.480958
16.363271	49.547689	4.491238	-0.002835	0.498047
21.685073	54.749491	4.496243	-0.003829	0.515627
24.634572	60.749969	4.501248	-0.004382	0.533630
25.880156	67.394412	4.506253	-0.004618	0.551928
28.211846	74.171607	4.511258	-0.005057	0.570469
30.622100	81.256663	4.516262	-0.005510	0.589214
32.684715	88.688255	4.521267	-0.005899	0.608056
34.565039	96.444297	4.526272	-0.006254	0.627002
36.973912	104.369659	4.531277	-0.006708	0.645981
39.638301	112.507119	4.536282	-0.007209	0.664976
41.140089	121.064925	4.541286	-0.007494	0.683892
43.432220	129.679277	4.546291	-0.007927	0.702703
46.105165	138.407339	4.551296	-0.008430	0.721385
48.172740	147.428881	4.556301	-0.008821	0.739956
50.717475	156.503864	4.561306	-0.009300	0.758334
52.745543	165.785489	4.566310	-0.009684	0.776488
55.371112	175.077753	4.571315	-0.010179	0.794438
58.042424	184.450243	4.576320	-0.010682	0.812147
59.662477	194.088190	4.581325	-0.010990	0.829613
61.433843	203.750839	4.586330	-0.011326	0.846806
63.441802	213.377188	4.591334	-0.011707	0.863664
64.895066	223.130417	4.596339	-0.011983	0.880246
66.311510	232.885735	4.601344	-0.012254	0.896513
68.101686	242.589648	4.606349	-0.012593	0.912511
70.294948	252.193146	4.611354	-0.013008	0.928186
72.306768	261.809170	4.616358	-0.013389	0.943570
73.995378	271.478136	4.621363	-0.013709	0.958699
75.882965	281.064629	4.626368	-0.014067	0.973522
77.814834	290.637887	4.631373	-0.014433	0.988113
80.258101	300.063152	4.636378	-0.014894	1.002406
82.831282	309.407140	4.641382	-0.015379	1.016412
83.739023	319.035496	4.646387	-0.015554	1.030219
85.516998	328.415375	4.651392	-0.015891	1.043709
87.330679	337.766168	4.656397	-0.016235	1.056994
88.993812	347.101614	4.661402	-0.016551	1.070056
90.465390	356.382850	4.666406	-0.016831	1.082844
92.401769	365.565625	4.671411	-0.017197	1.095458
93.883899	374.762475	4.676416	-0.017479	1.107843
95.192600	383.946696	4.681421	-0.017729	1.120036
97.142003	392.967730	4.686426	-0.018098	1.132029
99.096161	401.932358	4.691430	-0.018467	1.143824
100.663679	410.966047	4.696435	-0.018765	1.155502
101.455399	420.037152	4.701440	-0.018918	1.166945
102.833514	428.958930	4.706445	-0.019181	1.178215
103.904429	437.910303	4.711450	-0.019386	1.189350
105.217300	446.756669	4.716454	-0.019636	1.200305
106.406052	455.600543	4.721459	-0.019863	1.211132
107.385457	464.428208	4.726464	-0.020051	1.221801
109.073829	473.113282	4.731469	-0.020371	1.232351
110.545921	481.794867	4.736474	-0.020651	1.242764
111.353341	490.560575	4.741478	-0.020807	1.253057
112.112472	499.297877	4.746483	-0.020954	1.263224
112.627833	508.033656	4.751488	-0.021056	1.273261
114.006856	516.580188	4.756493	-0.021318	1.283171
114.919011	525.209354	4.761498	-0.021493	1.293008
116.297067	533.717555	4.766502	-0.021755	1.302723
117.474378	542.312105	4.771507	-0.021980	1.312424
118.880704	550.786384	4.776512	-0.022248	1.321964
119.375636	559.382230	4.781517	-0.022345	1.331400
120.657691	567.807366	4.786522	-0.022589	1.340728
121.503053	576.305350	4.791526	-0.022752	1.349991
122.629092	584.747012	4.796531	-0.022967	1.359181
123.072657	593.284569	4.801536	-0.023056	1.368289
123.781000	601.745531	4.806541	-0.023193	1.377303
124.679191	610.161318	4.811546	-0.023366	1.386244
125.697501	618.543637	4.816550	-0.023561	1.395113
126.694512	626.914415	4.821555	-0.023752	1.403910
127.130746	635.383028	4.826560	-0.023838	1.412657
128.112808	643.702335	4.831565	-0.024027	1.421290
129.387069	652.011630	4.836570	-0.024269	1.429909
129.492878	660.491267	4.841574	-0.024294	1.438454
130.661644	668.757548	4.846579	-0.024517	1.446910
131.537403	677.100290	4.851584	-0.024686	1.455344
132.554391	685.399771	4.856589	-0.024881	1.463709
133.742180	693.721569	4.861594	-0.025107	1.472076
134.788367	701.990822	4.866598	-0.025307	1.480322
135.445406	710.341982	4.871603	-0.025435	1.488539
136.122389	718.664875	4.876608	-0.025566	1.496686
136.561347	727.014051	4.881613	-0.025654	1.504777
137.176449	735.336966	4.886618	-0.025773	1.512827
137.827418	743.607192	4.891622	-0.025900	1.520789
138.874408	751.864249	4.896627	-0.026100	1.528758
139.910921	760.090465	4.901632	-0.026299	1.536655
140.731960	768.352248	4.906637	-0.026457	1.544512
141.555096	776.647438	4.911642	-0.026615	1.552360
141.802084	784.978264	4.916646	-0.026667	1.560115
142.681910	793.184261	4.921651	-0.026836	1.567810
143.839683	801.343078	4.926656	-0.027057	1.575466
144.342611	809.652756	4.931661	-0.027156	1.583125
145.032568	817.917878	4.936666	-0.027290	1.590735
145.488993	826.190297	4.941670	-0.027380	1.598280
146.519622	834.342530	4.946675	-0.027577	1.605765
147.059690	842.636312	4.951680	-0.027683	1.613271
147.875593	850.830876	4.956685	-0.027840	1.620693
148.118987	859.174299	4.961690	-0.027891	1.628131
148.967284	867.358042	4.966694	-0.028054	1.635480
149.903671	875.519440	4.971699	-0.028234	1.642789
151.020705	883.641002	4.976704	-0.028447	1.650055
152.012632	891.806510	4.981709	-0.028637	1.657310
153.462509	899.907502	4.986714	-0.028912	1.664540
154.059088	908.182043	4.991718	-0.029029	1.671771
154.774047	916.399564	4.996723	-0.029167	1.678938
155.615083	924.584252	5.001728	-0.029329	1.686063
156.074720	932.844985	5.006733	-0.029420	1.693171
157.350849	940.957382	5.011738	-0.029663	1.700233
158.241243	949.138161	5.016742	-0.029834	1.707272
158.857320	957.384752	5.021747	-0.029954	1.714301
160.000514	965.494555	5.026752	-0.030172	1.721255
160.957103	973.644008	5.031757	-0.030355	1.728190
162.158365	981.784042	5.036762	-0.030584	1.735121
163.463085	989.909007	5.041766	-0.030833	1.742025
164.706225	998.049209	5.046771	-0.031069	1.748905
165.861409	1006.199091	5.051776	-0.031290	1.755755
166.661323	1014.418521	5.056781	-0.031444	1.762590
167.982624	1022.566399	5.061786	-0.031695	1.769406
168.947737	1030.758018	5.066790	-0.031880	1.776185
170.155304	1038.911883	5.071795	-0.032110	1.782939
171.473451	1047.059165	5.076800	-0.032361	1.789675
172.703353	1055.227683	5.081805	-0.032595	1.796391
174.071407	1063.348934	5.086810	-0.032855	1.803062
175.319417	1071.474756	5.091814	-0.033093	1.809696
176.841875	1079.568669	5.096819	-0.033382	1.816314
177.499382	1087.823652	5.101824	-0.033509	1.822929
178.080868	1096.054019	5.106829	-0.033623	1.829491
178.765143	1104.262058	5.111834	-0.033756	1.836025
179.781425	1112.374181	5.116838	-0.033950	1.842500
180.414740	1120.594602	5.121843	-0.034073	1.848991
181.585740	1128.694341	5.126848	-0.034297	1.855429
182.082344	1136.906058	5.131853	-0.034394	1.861851
182.676579	1145.112826	5.136858	-0.034510	1.868259
183.700298	1153.207225	5.141862	-0.034706	1.874608
184.309712	1161.358921	5.146867	-0.034825	1.880932
184.890395	1169.534430	5.151872	-0.034938	1.887248
185.091013	1177.749042	5.156877	-0.034981	1.893530
185.982825	1185.839144	5.161882	-0.035152	1.899775
186.264771	1194.017421	5.166886	-0.035210	1.905997
186.939312	1202.165977	5.171891	-0.035341	1.912221
187.502808	1210.285561	5.176896	-0.035451	1.918390
188.328682	1218.359724	5.181901	-0.035610	1.924534
189.257155	1226.458322	5.186906	-0.035788	1.930689
189.599968	1234.630727	5.191910	-0.035857	1.936813
190.680458	1242.695274	5.196915	-0.036064	1.942920
191.683204	1250.782455	5.201920	-0.036256	1.949016
191.615037	1259.046621	5.206925	-0.036248	1.955104
192.677732	1267.079176	5.211930	-0.036451	1.961128
193.441317	1275.161572	5.216934	-0.036599	1.967136
193.673373	1283.387321	5.221939	-0.036647	1.973173
194.200583	1291.514908	5.226944	-0.036751	1.979152
195.030800	1299.557033	5.231949	-0.036911	1.985084
195.838238	1307.666411	5.236954	-0.037066	1.991044
196.761904	1315.716125	5.241958	-0.037243	1.996955
196.926783	1323.928443	5.246963	-0.037279	2.002884
197.346472	1332.082716	5.251968	-0.037363	2.008782
197.653590	1340.240031	5.256973	-0.037425	2.014652
198.582973	1348.280935	5.261978	-0.037603	2.020488
199.542965	1356.329916	5.266982	-0.037787	2.026315
200.209490	1364.474713	5.271987	-0.037917	2.032163
201.435561	1372.480232	5.276992	-0.038150	2.037954
202.366733	1380.541075	5.281997	-0.038329	2.043736
202.826778	1388.726488	5.287002	-0.038420	2.049541
203.411950	1396.854463	5.292006	-0.038534	2.055302
204.432623	1404.886997	5.297011	-0.038729	2.061024
205.576462	1412.947269	5.302016	-0.038947	2.066762
206.261374	1421.066876	5.307021	-0.039080	2.072479
207.158529	1429.191042	5.312026	-0.039253	2.078204
208.082583	1437.276109	5.317030	-0.039430	2.083889
209.359630	1445.324576	5.322035	-0.039673	2.089569
210.441113	1453.431063	5.327040	-0.039879	2.095253
211.522656	1461.482727	5.332045	-0.040086	2.100884
212.648974	1469.605199	5.337050	-0.040301	2.106552
213.732865	1477.704836	5.342054	-0.040508	2.112185
215.413301	1485.700784	5.347059	-0.040826	2.117791
216.749485	1493.743500	5.352064	-0.041080	2.123380
217.741155	1501.870030	5.357069	-0.041270	2.128976
218.893994	1509.978807	5.362074	-0.041490	2.134562
220.117372	1518.057782	5.367078	-0.041723	2.140119
220.726155	1526.232496	5.372083	-0.041842	2.145667
221.434493	1534.403345	5.377088	-0.041979	2.151207
222.830333	1542.411287	5.382093	-0.042244	2.156689
224.315843	1550.444029	5.387098	-0.042526	2.162183
226.159234	1558.428327	5.392102	-0.042874	2.167664
227.188466	1566.594222	5.397107	-0.043071	2.173174
228.462500	1574.706289	5.402112	-0.043313	2.178657
229.454592	1582.809796	5.407117	-0.043503	2.184094
230.916596	1590.885457	5.412122	-0.043781	2.189543
232.484107	1598.921630	5.417126	-0.044078	2.194962
233.698878	1606.996907	5.422131	-0.044309	2.200359
235.349762	1615.008167	5.427136	-0.044622	2.205742
236.252113	1623.167032	5.432141	-0.044795	2.211139
237.909074	1631.223307	5.437146	-0.045109	2.216525
239.133934	1639.305438	5.442150	-0.045342	2.221874
240.247888	1647.457443	5.447155	-0.045555	2.227246
241.119664	1655.624536	5.452160	-0.045722	2.232592
242.693002	1663.612737	5.457165	-0.046021	2.237873
243.962734	1671.711293	5.462170	-0.046262	2.243185
245.321606	1679.768931	5.467174	-0.046520	2.248466
246.219178	1687.923766	5.472179	-0.046693	2.253755
248.088465	1695.923222	5.477184	-0.047046	2.259019
249.608691	1703.973694	5.482189	-0.047334	2.264271
251.329953	1712.056888	5.487194	-0.047660	2.269550
253.403890	1720.089637	5.492198	-0.048051	2.274815
255.328196	1728.081098	5.497203	-0.048415	2.280028
256.926307	1736.154850	5.502208	-0.048718	2.285252
257.658959	1744.384983	5.507213	-0.048859	2.290487
259.225536	1752.426203	5.512218	-0.049156	2.295663
260.391148	1760.534562	5.517222	-0.049379	2.300835
262.335431	1768.499571	5.522227	-0.049746	2.305972
263.548410	1776.667735	5.527232	-0.049977	2.311161
264.710749	1784.753160	5.532237	-0.050199	2.316283
265.935357	1792.869949	5.537242	-0.050432	2.321418
266.880452	1800.957464	5.542246	-0.050613	2.326499
268.560383	1808.963033	5.547251	-0.050931	2.331581
269.665975	1817.101269	5.552256	-0.051142	2.336684
270.937923	1825.158053	5.557261	-0.051384	2.341740
272.804048	1833.192990	5.562266	-0.051737	2.346821
274.001593	1841.324576	5.567270	-0.051965	2.351894
275.912899	1849.295162	5.572275	-0.052326	2.356917
277.549419	1857.345732	5.577280	-0.052636	2.361954
279.233057	1865.385108	5.582285	-0.052955	2.366977
280.659825	1873.505309	5.587290	-0.053226	2.372018
282.037328	1881.591542	5.592294	-0.053487	2.377023
283.682778	1889.620567	5.597299	-0.053799	2.382004
285.168367	1897.701767	5.602304	-0.054081	2.386992
286.361859	1905.831327	5.607309	-0.054308	2.391976
286.878272	1914.060684	5.612314	-0.054410	2.396954
287.939881	1922.130559	5.617318	-0.054613	2.401870
288.983902	1930.187875	5.622323	-0.054812	2.406767
290.331541	1938.258442	5.627328	-0.055068	2.411686
291.480267	1946.318573	5.632333	-0.055287	2.416572
292.960956	1954.340262	5.637338	-0.055568	2.421452
294.452984	1962.348087	5.642342	-0.055851	2.426314
296.088449	1970.408373	5.647347	-0.056161	2.431208
297.696521	1978.457864	5.652352	-0.056466	2.436084
299.023695	1986.537082	5.657357	-0.056718	2.440945
300.062312	1994.648847	5.662362	-0.056917	2.445793
301.905308	2002.630201	5.667366	-0.057265	2.450617
303.133631	2010.755707	5.672371	-0.057499	2.455468
304.646429	2018.787647	5.677376	-0.057786	2.460276
305.829394	2026.833544	5.682381	-0.058011	2.465057
306.585747	2035.013583	5.687386	-0.058157	2.469874
307.039703	2043.145850	5.692390	-0.058247	2.474631
307.721111	2051.226039	5.697395	-0.058379	2.479366
307.941462	2059.379096	5.702400	-0.058426	2.484099
308.428485	2067.465182	5.707405	-0.058521	2.488805
308.482046	2075.643937	5.712410	-0.058537	2.493522
309.117856	2083.653056	5.717414	-0.058660	2.498176
309.233969	2091.759682	5.722419	-0.058687	2.502839
309.718782	2099.833177	5.727424	-0.058783	2.507501
309.785034	2107.948867	5.732429	-0.058800	2.512148
310.268030	2115.987743	5.737434	-0.058895	2.516773
310.390596	2124.062178	5.742438	-0.058923	2.521383
310.229771	2132.167660	5.747443	-0.058899	2.525982
311.159919	2140.139234	5.752448	-0.059077	2.530576
311.868752	2148.131153	5.757453	-0.059214	2.535157
311.849239	2156.289381	5.762458	-0.059216	2.539771
312.159694	2164.305365	5.767462	-0.059279	2.544320
312.017162	2172.483895	5.772467	-0.059258	2.548919
312.242937	2180.554297	5.777472	-0.059305	2.553476
312.908226	2188.494230	5.782477	-0.059434	2.557983
313.514520	2196.508205	5.787482	-0.059552	2.562520
314.249931	2204.533760	5.792486	-0.059694	2.567063
314.718284	2212.587183	5.797491	-0.059786	2.571596
315.320308	2220.668439	5.802496	-0.059904	2.576145
315.907795	2228.688736	5.807501	-0.060018	2.580651
315.731047	2236.874747	5.812506	-0.059991	2.585187
315.861258	2244.965644	5.817510	-0.060020	2.589684
316.554270	2253.046405	5.822515	-0.060154	2.594207
316.944067	2261.081170	5.827520	-0.060232	2.598676
317.424990	2269.038453	5.832525	-0.060327	2.603100
318.496306	2276.992042	5.837530	-0.060531	2.607556
318.800507	2285.095911	5.842534	-0.060593	2.612033
319.299501	2293.114989	5.847539	-0.060691	2.616470
319.888484	2301.164419	5.852544	-0.060806	2.620921
319.612313	2309.320762	5.857549	-0.060760	2.625365
320.276909	2317.316617	5.862554	-0.060889	2.629777
320.482129	2325.406530	5.867558	-0.060933	2.634202
320.798013	2333.428444	5.872563	-0.060997	2.638590
321.694630	2341.406726	5.877568	-0.061169	2.642986
322.171331	2349.440337	5.882573	-0.061263	2.647376
322.131673	2357.620485	5.887578	-0.061261	2.651804
322.771140	2365.625212	5.892582	-0.061385	2.656175
322.987658	2373.675825	5.897587	-0.061430	2.660535
323.531529	2381.732653	5.902592	-0.061537	2.664913
323.877942	2389.781961	5.907597	-0.061606	2.669267
324.252161	2397.866235	5.912602	-0.061681	2.673634
324.467147	2405.912907	5.917606	-0.061727	2.677963
325.219304	2413.884469	5.922611	-0.061872	2.682280
325.837044	2421.914334	5.927616	-0.061992	2.686613
326.216862	2429.970644	5.932621	-0.062068	2.690936
326.226797	2438.128428	5.937626	-0.062075	2.695284
326.864268	2446.104715	5.942630	-0.062199	2.699568
327.303524	2454.140386	5.947635	-0.062286	2.703863
327.489940	2462.228475	5.952640	-0.062326	2.708164
327.814333	2470.281621	5.957645	-0.062391	2.712448
328.495575	2478.282279	5.962650	-0.062523	2.716720
328.713452	2486.348661	5.967654	-0.062569	2.720991
329.295307	2494.339111	5.972659	-0.062683	2.725238
329.223558	2502.518662	5.977664	-0.062675	2.729536
329.584435	2510.530250	5.982669	-0.062747	2.733767
329.760887	2518.620572	5.987674	-0.062785	2.738020
330.204344	2526.623733	5.992678	-0.062873	2.742238
330.316255	2534.718379	5.997683	-0.062899	2.746477
330.839505	2542.753390	6.002688	-0.063002	2.750704
331.263382	2550.811657	6.007693	-0.063086	2.754930
331.871286	2558.814525	6.012698	-0.063204	2.759132
332.453679	2566.786061	6.017702	-0.063318	2.763309
332.367045	2574.914602	6.022707	-0.063307	2.767521
333.058824	2582.920945	6.027712	-0.063441	2.771710
333.821897	2590.895174	6.032717	-0.063588	2.775881
333.879647	2598.999752	6.037722	-0.063604	2.780070
334.615880	2606.955255	6.042726	-0.063746	2.784216
334.828327	2615.068696	6.047731	-0.063791	2.788406
335.382051	2623.109621	6.052736	-0.063899	2.792573
335.410848	2631.200369	6.057741	-0.063910	2.796728
335.976258	2639.226057	6.062746	-0.064020	2.800875
336.219202	2647.248953	6.067750	-0.064071	2.804996
336.409183	2655.313780	6.072755	-0.064111	2.809128
336.820822	2663.395532	6.077760	-0.064193	2.813277
337.110678	2671.428729	6.082765	-0.064252	2.817387
337.781835	2679.413834	6.087770	-0.064383	2.821489
337.949709	2687.492325	6.092774	-0.064419	2.825603
338.422509	2695.532821	6.097779	-0.064512	2.829709
339.114657	2703.531083	6.102784	-0.064646	2.833801
339.438710	2711.561893	6.107789	-0.064712	2.837881
339.562262	2719.676272	6.112794	-0.064740	2.841987
339.935576	2727.697102	6.117798	-0.064815	2.846054
340.281785	2735.737674	6.122803	-0.064884	2.850123
340.945024	2743.769362	6.127808	-0.065013	2.854200
341.078576	2751.848870	6.132813	-0.065043	2.858265
341.312142	2759.908672	6.137818	-0.065092	2.862319
342.121359	2767.865525	6.142822	-0.065248	2.866350
342.372420	2775.964644	6.147827	-0.065300	2.870414
343.162450	2783.961346	6.152832	-0.065452	2.874451
343.583964	2791.991222	6.157837	-0.065536	2.878478
343.721307	2800.072713	6.162842	-0.065566	2.882510
343.923338	2808.138229	6.167846	-0.065609	2.886531
344.472718	2816.132747	6.172851	-0.065717	2.890531
344.899610	2824.220410	6.177856	-0.065801	2.894565
345.072752	2832.283586	6.182861	-0.065839	2.898567
345.056026	2840.364020	6.187866	-0.065841	2.902561
345.140616	2848.405073	6.192870	-0.065862	2.906536
345.777682	2856.414790	6.197875	-0.065986	2.910520
345.913382	2864.546663	6.202880	-0.066016	2.914532
345.922681	2872.541805	6.207885	-0.066023	2.918463
346.584360	2880.502972	6.212890	-0.066151	2.922409
347.142694	2888.491763	6.217894	-0.066261	2.926356
347.335189	2896.542163	6.222899	-0.066302	2.930309
347.994634	2904.594994	6.227904	-0.066430	2.934283
347.924476	2912.664354	6.232909	-0.066422	2.938220
348.528533	2920.643724	6.237914	-0.066539	2.942144
349.035701	2928.692784	6.242918	-0.066639	2.946092
349.299992	2936.739618	6.247923	-0.066693	2.950020
349.672343	2944.818349	6.252928	-0.066768	2.953964
350.008742	2952.794789	6.257933	-0.066836	2.957851
350.682316	2960.815582	6.262938	-0.066966	2.961772
350.913896	2968.881724	6.267942	-0.067015	2.965687
351.681235	2976.826976	6.272947	-0.067163	2.969566
352.411527	2984.885445	6.277952	-0.067304	2.973492
352.222554	2993.054069	6.282957	-0.067274	2.977419
352.164750	3001.134229	6.287962	-0.067268	2.981305
352.200423	3009.184318	6.292966	-0.067280	2.985176
352.343838	3017.245044	6.297971	-0.067312	2.989052
352.951013	3025.224324	6.302976	-0.067430	2.992908
353.399131	3033.182930	6.307981	-0.067519	2.996742
353.285848	3041.313106	6.312986	-0.067503	3.000623
354.034229	3049.210918	6.317990	-0.067648	3.004433
353.863813	3057.384464	6.322995	-0.067621	3.008322
354.420659	3065.379222	6.328000	-0.067730	3.012158
355.188327	3073.328005	6.333005	-0.067878	3.015978
355.378179	3081.414741	6.338010	-0.067919	3.019829
355.362854	3089.499308	6.343014	-0.067921	3.023664
355.788133	3097.493699	6.348019	-0.068005	3.027474
356.408985	3105.532630	6.353024	-0.068126	3.031309
356.786926	3113.571198	6.358029	-0.068202	3.035127
357.041614	3121.584685	6.363034	-0.068254	3.038923
356.995990	3129.710607	6.368038	-0.068251	3.042752
357.501499	3137.694400	6.373043	-0.068350	3.046536
358.165744	3145.678511	6.378048	-0.068479	3.050323
358.534161	3153.736223	6.383053	-0.068553	3.054126
358.997689	3161.768342	6.388058	-0.068645	3.057916
359.513703	3169.819913	6.393062	-0.068746	3.061713
359.643736	3177.908944	6.398067	-0.068775	3.065505
360.327577	3185.915537	6.403072	-0.068908	3.069280
360.579209	3193.986196	6.408077	-0.068960	3.073059
361.324966	3201.959889	6.413082	-0.069104	3.076812
361.718713	3210.018709	6.418086	-0.069182	3.080583
361.833334	3218.005336	6.423091	-0.069209	3.084302
362.248900	3226.050298	6.428096	-0.069291	3.088059
362.290783	3234.129899	6.433101	-0.069305	3.091809
362.532400	3242.180141	6.438106	-0.069355	3.095550
363.563736	3250.074341	6.443110	-0.069552	3.099252
363.291512	3258.210641	6.448115	-0.069506	3.103000
363.845860	3266.215527	6.453120	-0.069615	3.106721
363.979723	3274.303236	6.458125	-0.069645	3.110457
364.466334	3282.297374	6.463130	-0.069741	3.114161
364.491243	3290.376235	6.468134	-0.069751	3.117878
364.777934	3298.377973	6.473139	-0.069809	3.121568
364.915315	3306.426069	6.478144	-0.069840	3.125268
365.097509	3314.462942	6.483149	-0.069879	3.128960
365.389400	3322.520980	6.488154	-0.069939	3.132662
365.490244	3330.603632	6.493158	-0.069963	3.136363
365.904523	3338.545045	6.498163	-0.070045	3.140008
366.686268	3346.528618	6.503168	-0.070196	3.143686
366.841524	3354.619609	6.508173	-0.070230	3.147380
367.562162	3362.636880	6.513178	-0.070369	3.151061
367.432165	3370.759451	6.518182	-0.070350	3.154747
367.572872	3378.747867	6.523187	-0.070381	3.158381
367.827013	3386.812942	6.528192	-0.070434	3.162050
368.488817	3394.760675	6.533197	-0.070562	3.165679
369.013651	3402.754741	6.538202	-0.070665	3.169319
368.806960	3410.910549	6.543206	-0.070632	3.172996
369.267368	3418.883403	6.548211	-0.070723	3.176616
370.064401	3426.877890	6.553216	-0.070877	3.180255
370.283792	3434.893602	6.558221	-0.070923	3.183875
370.179098	3443.017290	6.563226	-0.070908	3.187525
370.634285	3451.059990	6.568230	-0.070998	3.191158
370.740466	3459.077544	6.573235	-0.071023	3.194762
371.814657	3466.958087	6.578240	-0.071228	3.198341
372.050876	3475.038703	6.583245	-0.071278	3.201970
372.375478	3483.122234	6.588250	-0.071343	3.205599
372.022762	3491.254018	6.593254	-0.071283	3.209217
372.399291	3499.232103	6.598259	-0.071358	3.212794
372.768754	3507.283011	6.603264	-0.071432	3.216399
373.210812	3515.259072	6.608269	-0.071519	3.219969
373.091669	3523.349427	6.613274	-0.071503	3.223562
373.294453	3531.431636	6.618278	-0.071546	3.227162
373.528082	3539.436300	6.623283	-0.071594	3.230724
373.546802	3547.479346	6.628288	-0.071603	3.234290
373.761002	3555.443759	6.633293	-0.071648	3.237826
374.516333	3563.414201	6.638298	-0.071794	3.241383
374.631586	3571.467187	6.643302	-0.071820	3.244946
374.927932	3579.487383	6.648307	-0.071881	3.248497
375.393159	3587.535470	6.653312	-0.071973	3.252065
375.169075	3595.645467	6.658317	-0.071936	3.255627
375.388971	3603.614341	6.663322	-0.071982	3.259141
376.021177	3611.597775	6.668326	-0.072105	3.262675
376.002776	3619.670308	6.673331	-0.072107	3.266218
376.386339	3627.704514	6.678336	-0.072183	3.269756
376.480156	3635.759337	6.683341	-0.072206	3.273287
377.022394	3643.720995	6.688346	-0.072312	3.276792
377.339286	3651.754295	6.693350	-0.072376	3.280316
377.834555	3659.699924	6.698355	-0.072474	3.283805
378.158873	3667.804532	6.703360	-0.072539	3.287352
378.463279	3675.827373	6.708365	-0.072601	3.290859
378.460876	3683.924882	6.713370	-0.072606	3.294382
378.649568	3691.991443	6.718374	-0.072646	3.297896
379.393696	3699.951657	6.723379	-0.072790	3.301382
379.394175	3708.041870	6.728384	-0.072795	3.304891
379.694024	3716.063950	6.733389	-0.072856	3.308378
379.911048	3724.112203	6.738394	-0.072902	3.311870
380.328662	3732.096147	6.743398	-0.072985	3.315339
380.417863	3740.107235	6.748403	-0.073007	3.318802
380.922180	3748.132346	6.753408	-0.073106	3.322284
381.345806	3756.150134	6.758413	-0.073190	3.325756
381.090925	3764.249236	6.763418	-0.073148	3.329233
381.554786	3772.260903	6.768422	-0.073239	3.332697
382.025356	3780.257277	6.773427	-0.073332	3.336151
382.208570	3788.286851	6.778432	-0.073371	3.339604
382.049536	3796.344825	6.783437	-0.073347	3.343053
382.584857	3804.344094	6.788442	-0.073452	3.346499
383.060251	3812.384150	6.793446	-0.073545	3.349957
383.030937	3820.423631	6.798451	-0.073545	3.353392
383.712446	3828.415046	6.803456	-0.073677	3.356830
384.184645	3836.395168	6.808461	-0.073770	3.360251
384.242300	3844.444667	6.813466	-0.073786	3.363683
384.602664	3852.482734	6.818470	-0.073859	3.367118
384.687535	3860.563347	6.823475	-0.073880	3.370557
384.875800	3868.609496	6.828480	-0.073920	3.373982
384.907695	3876.661213	6.833485	-0.073931	3.377400
385.472755	3884.636905	6.838490	-0.074041	3.380802
385.969666	3892.614958	6.843494	-0.074139	3.384198
386.172358	3900.656010	6.848499	-0.074182	3.387608
386.790275	3908.739986	6.853504	-0.074302	3.391047
386.722981	3916.829502	6.858509	-0.074295	3.394460
386.742260	3924.855339	6.863514	-0.074304	3.397845
387.565933	3932.806083	6.868518	-0.074462	3.401225
387.847795	3940.757595	6.873523	-0.074520	3.404582
388.077310	3948.844823	6.878528	-0.074568	3.407991
388.213672	3956.907224	6.883533	-0.074598	3.411383
388.962791	3964.833888	6.888538	-0.074743	3.414736
388.752556	3972.984060	6.893542	-0.074709	3.418145
388.732267	3981.004813	6.898547	-0.074711	3.421504
389.109888	3988.985278	6.903552	-0.074786	3.424856
389.853560	3996.970894	6.908557	-0.074930	3.428220
390.001393	4005.041922	6.913562	-0.074962	3.431596
390.252719	4013.072707	6.918566	-0.075014	3.434955
390.803397	4021.040993	6.923571	-0.075122	3.438295
391.404280	4029.073916	6.928576	-0.075239	3.441660
391.287030	4037.139585	6.933581	-0.075223	3.445011
391.679988	4045.154607	6.938586	-0.075301	3.448355
391.947877	4053.236006	6.943590	-0.075356	3.451719
392.172273	4061.243872	6.948595	-0.075403	3.455047
392.603190	4069.266852	6.953600	-0.075488	3.458386
392.359874	4077.370011	6.958605	-0.075448	3.461732
392.450248	4085.382815	6.963610	-0.075470	3.465048
392.997141	4093.384521	6.968614	-0.075577	3.468372
393.479798	4101.355462	6.973619	-0.075672	3.471678
393.951608	4109.386619	6.978624	-0.075765	3.475005
394.558186	4117.334491	6.983629	-0.075883	3.478299
394.581253	4125.445517	6.988634	-0.075893	3.481638
394.627366	4133.491849	6.993638	-0.075907	3.484948
394.887153	4141.485461	6.998643	-0.075960	3.488240
395.060853	4149.568961	7.003648	-0.075998	3.491562
395.530280	4157.540004	7.008653	-0.076090	3.494845
396.198372	4165.517520	7.013658	-0.076220	3.498134
396.369226	4173.613145	7.018662	-0.076257	3.501452
396.238303	4181.670792	7.023667	-0.076238	3.504742
396.996504	4189.636984	7.028672	-0.076384	3.508020
397.671691	4197.661132	7.033677	-0.076515	3.511315
397.848491	4205.696883	7.038682	-0.076553	3.514597
398.350006	4213.714126	7.043686	-0.076652	3.517878
398.860456	4221.716134	7.048691	-0.076752	3.521149
398.970669	4229.764590	7.053696	-0.076778	3.524424
399.288662	4237.797575	7.058701	-0.076842	3.527697
399.984020	4245.814409	7.063706	-0.076977	3.530971
399.938490	4253.876069	7.068710	-0.076973	3.534237
399.969583	4261.946997	7.073715	-0.076984	3.537507
400.623627	4269.941369	7.078720	-0.077111	3.540761
400.606323	4277.939879	7.083725	-0.077113	3.543994
400.939635	4285.982370	7.088730	-0.077181	3.547252
401.074254	4294.041339	7.093734	-0.077211	3.550508
401.850059	4302.038198	7.098739	-0.077361	3.553755
402.316598	4310.048305	7.103744	-0.077453	3.556995
401.688774	4318.150101	7.108749	-0.077341	3.560235
401.830553	4326.109365	7.113754	-0.077372	3.563439
402.423984	4334.093272	7.118758	-0.077488	3.566664
402.561154	4342.111854	7.123763	-0.077519	3.569885
403.157226	4350.134629	7.128768	-0.077635	3.573119
403.263557	4358.221722	7.133773	-0.077660	3.576361
403.242812	4366.230427	7.138778	-0.077661	3.579566
403.853976	4374.237747	7.143782	-0.077780	3.582785
404.173459	4382.234240	7.148787	-0.077845	3.585988
403.674637	4390.380549	7.153792	-0.077757	3.589225
404.456921	4398.315228	7.158797	-0.077908	3.592411
404.549330	4406.390238	7.163802	-0.077931	3.595631
404.651426	4414.392563	7.168806	-0.077955	3.598819
404.894770	4422.405872	7.173811	-0.078005	3.602012
405.760119	4430.328482	7.178816	-0.078171	3.605185
405.575039	4438.447213	7.183821	-0.078142	3.608402
405.728239	4446.519492	7.188826	-0.078176	3.611608
406.194040	4454.515763	7.193830	-0.078268	3.614789
406.306559	4462.541568	7.198835	-0.078294	3.617970
406.761189	4470.608375	7.203840	-0.078384	3.621173
406.989677	4478.554874	7.208845	-0.078432	3.624320
407.906854	4486.520143	7.213850	-0.078607	3.627491
407.625140	4494.658119	7.218854	-0.078560	3.630693
407.594104	4502.687887	7.223859	-0.078560	3.633857
408.041339	4510.719340	7.228864	-0.078648	3.637032
408.071856	4518.723138	7.233869	-0.078659	3.640181
408.479731	4526.652495	7.238874	-0.078740	3.643310
409.458998	4534.602818	7.243878	-0.078928	3.646459
409.334508	4542.723705	7.248883	-0.078910	3.649642
409.596956	4550.750529	7.253888	-0.078964	3.652797
409.773059	4558.835877	7.258893	-0.079002	3.655968
410.125740	4566.778810	7.263898	-0.079073	3.659087
410.304097	4574.863757	7.268902	-0.079111	3.662253
410.151975	4582.900260	7.273907	-0.079088	3.665389
410.736884	4590.931251	7.278912	-0.079202	3.668540
410.574006	4598.994322	7.283917	-0.079177	3.671680
410.737472	4606.977772	7.288922	-0.079212	3.674795
411.516613	4614.942099	7.293926	-0.079363	3.677917
411.880483	4622.951445	7.298931	-0.079436	3.681043
411.774298	4631.022168	7.303936	-0.079421	3.684177
412.210559	4639.045323	7.308941	-0.079507	3.687304
412.653333	4647.063785	7.313946	-0.079595	3.690427
413.050568	4655.084251	7.318950	-0.079674	3.693547
413.155071	4663.132126	7.323955	-0.079699	3.696667
413.680341	4671.098995	7.328960	-0.079802	3.699764
413.858674	4679.138723	7.333965	-0.079840	3.702878
413.867507	4687.199809	7.338970	-0.079847	3.705992
413.668777	4695.311382	7.343974	-0.079815	3.709119
414.239118	4703.290623	7.348979	-0.079927	3.712211
414.919093	4711.301159	7.353984	-0.080058	3.715316
415.011547	4719.281067	7.358989	-0.080081	3.718391
415.288567	4727.313985	7.363994	-0.080138	3.721488
415.896175	4735.244388	7.368998	-0.080256	3.724552
416.010713	4743.284449	7.374003	-0.080282	3.727643
416.440980	4751.343296	7.379008	-0.080368	3.730747
415.887592	4759.480868	7.384013	-0.080270	3.733854
416.792883	4767.361290	7.389018	-0.080444	3.736895
417.148648	4775.425852	7.394022	-0.080515	3.739992
417.119937	4783.450068	7.399027	-0.080515	3.743060
417.587742	4791.472812	7.404032	-0.080607	3.746138
417.720610	4799.515541	7.409037	-0.080637	3.749212
418.149948	4807.533000	7.414042	-0.080722	3.752282
418.175101	4815.631984	7.419046	-0.080732	3.755370
418.819707	4823.500929	7.424051	-0.080857	3.758383
419.053351	4831.598473	7.429056	-0.080906	3.761471
419.480396	4839.560061	7.434061	-0.080991	3.764509
419.467568	4847.619912	7.439066	-0.080993	3.767571
419.817847	4855.687527	7.444070	-0.081064	3.770643
419.621071	4863.742386	7.449075	-0.081032	3.773694
420.218306	4871.709973	7.454080	-0.081149	3.776728
420.728039	4879.677275	7.459085	-0.081249	3.779758
421.300543	4887.681996	7.464090	-0.081361	3.782800
421.320669	4895.802500	7.469094	-0.081370	3.785872
421.681434	4903.748398	7.474099	-0.081442	3.788882
421.943845	4911.823431	7.479104	-0.081496	3.791937
422.443551	4919.833538	7.484109	-0.081594	3.794970
422.458462	4927.864750	7.489114	-0.081602	3.797997
422.945099	4935.873882	7.494118	-0.081698	3.801025
423.658317	4943.765588	7.499123	-0.081836	3.804010
424.083207	4951.856386	7.504128	-0.081920	3.807062
424.077480	4959.915623	7.509133	-0.081924	3.810090
424.138350	4967.997271	7.514138	-0.081941	3.813125
424.219714	4976.106655	7.519142	-0.081961	3.816169
424.475772	4984.013048	7.524147	-0.082014	3.819138
424.787784	4992.033322	7.529152	-0.082077	3.822148
424.569334	5000.105472	7.534157	-0.082042	3.825164
424.373115	5008.195965	7.539162	-0.082011	3.828185
424.604478	5016.219287	7.544166	-0.082059	3.831188
424.710168	5024.145067	7.549171	-0.082084	3.834149
425.257933	5032.181964	7.554176	-0.082191	3.837159
425.590153	5040.139858	7.559181	-0.082258	3.840132
424.877519	5048.280903	7.564186	-0.082130	3.843149
425.776828	5056.223755	7.569190	-0.082303	3.846124
426.359587	5064.157697	7.574195	-0.082417	3.849087
426.689106	5072.243596	7.579200	-0.082483	3.852099
427.140531	5080.230616	7.584205	-0.082572	3.855074
426.729835	5088.325932	7.589210	-0.082501	3.858068
426.851619	5096.414126	7.594214	-0.082529	3.861069
426.901113	5104.370250	7.599219	-0.082543	3.864017
427.120192	5112.422530	7.604224	-0.082589	3.867002
427.759193	5120.388404	7.609229	-0.082714	3.869961
427.956585	5128.491755	7.614234	-0.082756	3.872960
427.950359	5136.611096	7.619238	-0.082760	3.875958
427.975187	5144.496315	7.624243	-0.082769	3.878868
427.781818	5152.573154	7.629248	-0.082739	3.881842
428.582344	5160.445515	7.634253	-0.082893	3.884759
428.653205	5168.487110	7.639258	-0.082911	3.887721
428.877411	5176.571507	7.644262	-0.082958	3.890699
429.290574	5184.539774	7.649267	-0.083040	3.893636
429.803518	5192.570061	7.654272	-0.083141	3.896596
429.761614	5200.583867	7.659277	-0.083138	3.899536
430.218651	5208.569216	7.664282	-0.083229	3.902474
430.463650	5216.648851	7.669286	-0.083279	3.905439
430.498563	5224.623986	7.674291	-0.083291	3.908360
430.748056	5232.691857	7.679296	-0.083343	3.911317
431.223398	5240.679663	7.684301	-0.083436	3.914247
431.720740	5248.639163	7.689306	-0.083534	3.917164
431.847888	5256.721819	7.694310	-0.083563	3.920117
431.757880	5264.766361	7.699315	-0.083551	3.923050
432.098599	5272.818394	7.704320	-0.083620	3.925992
432.331821	5280.819617	7.709325	-0.083669	3.928911
432.714588	5288.826871	7.714330	-0.083745	3.931832
433.125542	5296.872288	7.719334	-0.083827	3.934766
433.328748	5304.856372	7.724339	-0.083870	3.937671
433.305352	5312.911378	7.729344	-0.083871	3.940596
433.995620	5320.870532	7.734349	-0.084004	3.943497
434.146567	5328.920115	7.739354	-0.084038	3.946418
434.219002	5336.990916	7.744358	-0.084056	3.949344
434.019840	5345.098694	7.749363	-0.084025	3.952276
434.863427	5352.981323	7.754368	-0.084187	3.955143
435.055430	5360.992497	7.759373	-0.084228	3.958043
435.252745	5369.012829	7.764378	-0.084270	3.960944
435.248742	5377.081140	7.769382	-0.084274	3.963856
435.523676	5385.066269	7.774387	-0.084330	3.966742
435.703448	5393.068956	7.779392	-0.084369	3.969630
436.010931	5401.140651	7.784397	-0.084431	3.972542
436.093414	5409.140035	7.789402	-0.084452	3.975423
436.843227	5417.092800	7.794406	-0.084597	3.978297
436.233401	5425.269644	7.799411	-0.084488	3.981225
436.565040	5433.191121	7.804416	-0.084555	3.984075
436.943203	5441.218869	7.809421	-0.084631	3.986963
437.227550	5449.209201	7.814426	-0.084689	3.989833
437.817223	5457.241396	7.819430	-0.084804	3.992722
437.581457	5465.283127	7.824435	-0.084765	3.995597
437.852865	5473.272521	7.829440	-0.084821	3.998461
437.760634	5481.383597	7.834445	-0.084809	4.001360
437.920224	5489.284179	7.839450	-0.084844	4.004185
437.983799	5497.416193	7.844454	-0.084861	4.007090
438.139867	5505.394909	7.849459	-0.084895	4.009940
438.375420	5513.418610	7.854464	-0.084944	4.012804
438.649668	5521.464774	7.859469	-0.085001	4.015676
439.317225	5529.340851	7.864474	-0.085130	4.018491
439.743013	5537.459403	7.869478	-0.085214	4.021386
440.139838	5545.364820	7.874483	-0.085293	4.024203
440.047919	5553.536354	7.879488	-0.085282	4.027105
440.241089	5561.573313	7.884493	-0.085323	4.029961
440.995472	5569.538004	7.889498	-0.085468	4.032799
441.331808	5577.599589	7.894502	-0.085536	4.035662
441.774689	5585.550335	7.899507	-0.085624	4.038485
442.052313	5593.590045	7.904512	-0.085681	4.041336
442.236874	5601.571687	7.909517	-0.085720	4.044162
442.297219	5609.638675	7.914522	-0.085737	4.047015
443.083242	5617.605340	7.919526	-0.085888	4.049841
443.027461	5625.661502	7.924531	-0.085883	4.052684
443.328351	5633.670639	7.929536	-0.085944	4.055514
443.664388	5641.698160	7.934541	-0.086012	4.058348
443.680801	5649.786863	7.939546	-0.086020	4.061198
443.826966	5657.735520	7.944550	-0.086053	4.063998
444.047222	5665.773579	7.949555	-0.086099	4.066829
444.345340	5673.811370	7.954560	-0.086160	4.069659
444.614227	5681.847232	7.959565	-0.086215	4.072485
444.283557	5689.863285	7.964570	-0.086158	4.075294
444.894977	5697.849771	7.969574	-0.086277	4.078104
444.621563	5705.974212	7.974579	-0.086232	4.080948
445.380923	5713.834050	7.979584	-0.086378	4.083713
445.208692	5721.942283	7.984589	-0.086351	4.086548
445.871658	5729.857511	7.989594	-0.086480	4.089327
445.930126	5737.966608	7.994598	-0.086496	4.092162
445.943533	5745.985740	7.999603	-0.086504	4.094963
446.448853	5754.001204	8.004608	-0.086603	4.097768
446.505674	5762.042233	8.009613	-0.086619	4.100574
446.658487	5769.992675	8.014618	-0.086652	4.103348
446.676599	5778.074969	8.019622	-0.086661	4.106163
447.399715	5786.035262	8.024627	-0.086801	4.108945
447.536254	5794.084573	8.029632	-0.086831	4.111747
447.928756	5802.102429	8.034637	-0.086910	4.114539
448.088368	5810.086464	8.039642	-0.086945	4.117315
448.661937	5818.094040	8.044646	-0.087057	4.120103
448.651653	5826.115483	8.049651	-0.087060	4.122885
448.760977	5834.155758	8.054656	-0.087085	4.125674
448.582550	5842.267542	8.059661	-0.087057	4.128482
448.892061	5850.238988	8.064666	-0.087120	4.131246
448.843958	5858.287243	8.069670	-0.087116	4.134030
448.907007	5866.315038	8.074675	-0.087133	4.136806
449.358332	5874.263179	8.079680	-0.087222	4.139558
449.656843	5882.278590	8.084685	-0.087283	4.142330
449.549695	5890.280176	8.089690	-0.087268	4.145089
450.187062	5898.308452	8.094694	-0.087392	4.147866
450.226784	5906.324470	8.099699	-0.087405	4.150628
450.278470	5914.365367	8.104704	-0.087420	4.153398
450.613972	5922.395894	8.109709	-0.087487	4.156165
451.051034	5930.317450	8.114714	-0.087574	4.158895
451.164447	5938.446883	8.119718	-0.087600	4.161690
451.191681	5946.393041	8.124723	-0.087610	4.164419
451.497227	5954.449182	8.129728	-0.087673	4.167188
451.724033	5962.457146	8.134733	-0.087720	4.169937
451.983229	5970.477556	8.139738	-0.087773	4.172689
452.398835	5978.526168	8.144742	-0.087856	4.175451
452.643107	5986.528769	8.149747	-0.087907	4.178193
452.514792	5994.619932	8.154752	-0.087888	4.180959
452.767377	6002.612851	8.159757	-0.087940	4.183694
452.760417	6010.642849	8.164762	-0.087944	4.186437
452.938053	6018.671837	8.169766	-0.087982	4.189180
454.029431	6026.612098	8.174771	-0.088191	4.191902
453.928520	6034.718072	8.179776	-0.088177	4.194664
453.931762	6042.722291	8.184781	-0.088183	4.197391
454.564833	6050.645666	8.189786	-0.088306	4.200096
454.812838	6058.704624	8.194790	-0.088357	4.202841
454.870771	6066.697134	8.199795	-0.088373	4.205559
455.234579	6074.664641	8.204800	-0.088446	4.208271
455.420249	6082.763699	8.209805	-0.088486	4.211023
455.738394	6090.753435	8.214810	-0.088550	4.213738
455.926545	6098.817091	8.219814	-0.088591	4.216475
456.473701	6106.751154	8.224819	-0.088698	4.219170
456.936800	6114.808442	8.229824	-0.088789	4.221904
456.289344	6122.883037	8.234829	-0.088674	4.224630
456.803513	6130.840391	8.239834	-0.088775	4.227327
457.028486	6138.922898	8.244838	-0.088822	4.230061
457.120154	6146.917784	8.249843	-0.088844	4.232763
457.354492	6154.899568	8.254848	-0.088893	4.235460
457.705264	6162.923721	8.259853	-0.088963	4.238171
458.325072	6170.894066	8.264858	-0.089084	4.240865
458.579484	6178.889082	8.269862	-0.089136	4.243561
458.596632	6186.977080	8.274867	-0.089145	4.246285
459.058742	6194.957762	8.279872	-0.089236	4.248975
459.412655	6203.012827	8.284877	-0.089307	4.251688
458.917812	6211.092499	8.289882	-0.089220	4.254398
459.559363	6219.063134	8.294886	-0.089345	4.257081
459.862855	6227.062804	8.299891	-0.089406	4.259769
460.392464	6235.009955	8.304896	-0.089510	4.262440
460.358861	6243.106951	8.309901	-0.089509	4.265154
460.202836	6251.195787	8.314906	-0.089485	4.267863
460.649518	6259.183192	8.319910	-0.089574	4.270541
460.961220	6267.142237	8.324915	-0.089637	4.273207
460.933306	6275.245637	8.329920	-0.089637	4.275916
461.014968	6283.195078	8.334925	-0.089657	4.278573
460.985935	6291.274102	8.339930	-0.089657	4.281271
461.655381	6299.164252	8.344934	-0.089787	4.283910
462.139375	6307.209683	8.349939	-0.089882	4.286598
462.326870	6315.176488	8.354944	-0.089922	4.289255
462.783979	6323.268655	8.359949	-0.090012	4.291955
462.665351	6331.301561	8.364954	-0.089996	4.294628
462.825239	6339.341523	8.369958	-0.090031	4.297304
463.277913	6347.308511	8.374963	-0.090120	4.299957
463.261959	6355.378231	8.379968	-0.090122	4.302638
463.172461	6363.441701	8.384973	-0.090111	4.305315
463.253656	6371.390074	8.389978	-0.090131	4.307953
463.986320	6379.422038	8.394982	-0.090273	4.310623
464.406161	6387.383255	8.399987	-0.090356	4.313265
464.530119	6395.449272	8.404992	-0.090384	4.315938
464.684484	6403.405445	8.409997	-0.090418	4.318573
464.883677	6411.488172	8.415002	-0.090460	4.321249
465.206204	6419.408649	8.420006	-0.090526	4.323870
465.753351	6427.464774	8.425011	-0.090633	4.326536
465.623646	6435.443878	8.430016	-0.090614	4.329170
466.120973	6443.527475	8.435021	-0.090712	4.331841
466.445276	6451.494387	8.440026	-0.090777	4.334471
466.686694	6459.579064	8.445030	-0.090827	4.337138
467.168909	6467.519157	8.450035	-0.090922	4.339757
466.967329	6475.584238	8.455040	-0.090890	4.342410
467.249484	6483.587205	8.460045	-0.090948	4.345045
467.419051	6491.586284	8.465050	-0.090984	4.347676
467.495487	6499.681699	8.470054	-0.091004	4.350337
467.408608	6507.730557	8.475059	-0.090993	4.352979
467.828479	6515.713236	8.480064	-0.091076	4.355602
468.217346	6523.676820	8.485069	-0.091154	4.358217
467.867171	6531.741268	8.490074	-0.091094	4.360858
468.643611	6539.661585	8.495078	-0.091243	4.363458
468.818360	6547.737009	8.500083	-0.091281	4.366103
469.241440	6555.686222	8.505088	-0.091365	4.368706
469.144135	6563.854565	8.510093	-0.091352	4.371377
469.041260	6571.862656	8.515098	-0.091338	4.373993
469.771970	6579.869087	8.520102	-0.091479	4.376613
469.772934	6587.820671	8.525107	-0.091485	4.379208
470.090902	6595.830977	8.530112	-0.091549	4.381823
470.118137	6603.881639	8.535117	-0.091559	4.384448
469.983077	6611.938397	8.540122	-0.091539	4.387072
470.304488	6619.968082	8.545126	-0.091604	4.389688
470.498206	6627.998424	8.550131	-0.091646	4.392303
470.905638	6635.942200	8.555136	-0.091727	4.394889
470.985990	6644.056460	8.560141	-0.091747	4.397526
471.054022	6652.052799	8.565146	-0.091765	4.400124
471.344612	6660.025761	8.570151	-0.091824	4.402714
471.462858	6668.047101	8.575155	-0.091851	4.405317
471.917498	6676.096088	8.580160	-0.091941	4.407930
472.357725	6684.071272	8.585165	-0.092028	4.410517
472.158449	6692.136817	8.590170	-0.091996	4.413128
472.241248	6700.240756	8.595175	-0.092017	4.415751
472.444443	6708.167914	8.600179	-0.092060	4.418316
472.659009	6716.200038	8.605184	-0.092105	4.420914
473.136614	6724.169733	8.610189	-0.092199	4.423492
473.199129	6732.230474	8.615194	-0.092216	4.426095
473.619255	6740.260126	8.620199	-0.092299	4.428688
473.691225	6748.313862	8.625203	-0.092318	4.431286
474.022077	6756.250979	8.630208	-0.092385	4.433846
474.187121	6764.344741	8.635213	-0.092421	4.436454
474.466639	6772.277617	8.640218	-0.092478	4.439010
475.528679	6780.291433	8.645223	-0.092681	4.441593
475.834454	6788.237376	8.650227	-0.092743	4.444150
476.046879	6796.297291	8.655232	-0.092788	4.446741
476.257677	6804.327993	8.660237	-0.092832	4.449322
476.359045	6812.410776	8.665242	-0.092856	4.451917
476.761307	6820.364508	8.670247	-0.092936	4.454470
477.175022	6828.444561	8.675251	-0.093018	4.457063
477.024869	6836.427287	8.680256	-0.092996	4.459620
477.219133	6844.511185	8.685261	-0.093037	4.462209
477.402096	6852.410728	8.690266	-0.093076	4.464739
477.666080	6860.500210	8.695271	-0.093131	4.467327
477.714113	6868.536798	8.700275	-0.093145	4.469897
478.294615	6876.509495	8.705280	-0.093258	4.472447
478.269868	6884.561281	8.710285	-0.093259	4.475018
479.095290	6892.468933	8.715290	-0.093417	4.477544
479.295485	6900.549773	8.720295	-0.093460	4.480123
478.804870	6908.619356	8.725299	-0.093374	4.482693
479.133711	6916.561916	8.730304	-0.093440	4.485225
479.395133	6924.664873	8.735309	-0.093494	4.487806
480.126796	6932.578675	8.740314	-0.093635	4.490327
480.207440	6940.624514	8.745319	-0.093656	4.492886
480.178684	6948.698816	8.750323	-0.093655	4.495452
480.302043	6956.696407	8.755328	-0.093684	4.497993
480.751142	6964.636983	8.760333	-0.093772	4.500516
480.936800	6972.679509	8.765338	-0.093812	4.503068
481.477909	6980.694378	8.770343	-0.093918	4.505612
481.653501	6988.723689	8.775347	-0.093956	4.508157
481.648354	6996.744659	8.780352	-0.093960	4.510698
482.102226	7004.758687	8.785357	-0.094050	4.513236
481.922517	7012.787539	8.790362	-0.094022	4.515776
482.257427	7020.747789	8.795367	-0.094089	4.518294
482.451232	7028.768286	8.800371	-0.094130	4.520829
482.921189	7036.722620	8.805376	-0.094223	4.523343
483.164362	7044.859694	8.810381	-0.094274	4.525913
482.783210	7052.867407	8.815386	-0.094208	4.528438
482.983483	7060.925960	8.820391	-0.094250	4.530980
483.243140	7068.889535	8.825395	-0.094304	4.533490
483.676907	7076.869097	8.830400	-0.094390	4.536005
483.967738	7084.907978	8.835405	-0.094449	4.538536
484.003263	7092.955445	8.840410	-0.094461	4.541068
484.778067	7100.863758	8.845415	-0.094610	4.543556
484.475373	7108.955615	8.850419	-0.094559	4.546099
484.901141	7116.930309	8.855424	-0.094644	4.548604
485.130468	7125.041277	8.860429	-0.094691	4.551151
484.814022	7133.005325	8.865434	-0.094638	4.553649
484.754559	7141.110363	8.870439	-0.094632	4.556190
485.001946	7148.986753	8.875443	-0.094683	4.558659
485.070142	7157.041120	8.880448	-0.094701	4.561182
485.345094	7165.065812	8.885453	-0.094757	4.563695
485.771516	7173.078187	8.890458	-0.094842	4.566202
486.452005	7181.001828	8.895463	-0.094974	4.568681
486.241256	7189.171728	8.900467	-0.094940	4.571234
486.896017	7197.065623	8.905472	-0.095067	4.573701
487.484594	7205.141445	8.910477	-0.095182	4.576223
487.933503	7213.076504	8.915482	-0.095270	4.578699
487.959619	7221.207295	8.920487	-0.095280	4.581234
487.555569	7229.185205	8.925491	-0.095210	4.583720
487.557734	7237.242758	8.930496	-0.095216	4.586230
488.037000	7245.291754	8.935501	-0.095310	4.588736
487.896104	7253.309614	8.940506	-0.095289	4.591231
488.469570	7261.211657	8.945511	-0.095401	4.593689
488.649600	7269.290351	8.950515	-0.095440	4.596200
488.782544	7277.259088	8.955520	-0.095470	4.598675
489.237482	7285.312657	8.960525	-0.095560	4.601176
489.012635	7293.259040	8.965530	-0.095523	4.603641
489.286977	7301.338150	8.970535	-0.095579	4.606147
489.798676	7309.342592	8.975539	-0.095680	4.608628
489.568454	7317.387549	8.980544	-0.095642	4.611120
489.805682	7325.426707	8.985549	-0.095691	4.613609
489.760580	7333.455713	8.990554	-0.095688	4.616094
489.831233	7341.407046	8.995559	-0.095707	4.618553
490.086288	7349.397728	9.000563	-0.095759	4.621023
490.525888	7357.312690	9.005568	-0.095846	4.623469
490.995686	7365.432238	9.010573	-0.095939	4.625976
491.175032	7373.406894	9.015578	-0.095977	4.628437
491.256622	7381.466944	9.020583	-0.095998	4.630923
491.414587	7389.457371	9.025587	-0.096032	4.633386
491.023090	7397.606381	9.030592	-0.095965	4.635897
491.849922	7405.470439	9.035597	-0.096124	4.638319
492.087288	7413.500247	9.040602	-0.096173	4.640790
492.260528	7421.513103	9.045607	-0.096211	4.643255
492.508697	7429.569938	9.050611	-0.096262	4.645732
492.297315	7437.606503	9.055616	-0.096228	4.648202
492.520537	7445.620166	9.060621	-0.096275	4.650663
492.699075	7453.586237	9.065626	-0.096313	4.653108
492.964342	7461.668650	9.070631	-0.096368	4.655587
493.085409	7469.647325	9.075635	-0.096395	4.658034
493.446370	7477.634707	9.080640	-0.096468	4.660481
493.580610	7485.682106	9.085645	-0.096498	4.662946
493.619273	7493.656107	9.090650	-0.096510	4.665387
493.914741	7501.717537	9.095655	-0.096570	4.667854
493.996296	7509.772634	9.100659	-0.096591	4.670317
494.361208	7517.738754	9.105664	-0.096664	4.672751
494.469809	7525.865897	9.110669	-0.096689	4.675234
494.458234	7533.822155	9.115674	-0.096692	4.677663
494.811191	7541.790865	9.120679	-0.096763	4.680095
495.400328	7549.721653	9.125683	-0.096878	4.682513
495.674907	7557.688441	9.130688	-0.096934	4.684941
495.493529	7565.864812	9.135693	-0.096906	4.687433
495.947650	7573.837746	9.140698	-0.096996	4.689860
496.263893	7581.861622	9.145703	-0.097060	4.692302
496.532295	7589.856751	9.150707	-0.097115	4.694733
496.761032	7597.881634	9.155712	-0.097163	4.697173
497.055101	7605.893625	9.160717	-0.097223	4.699607
496.814996	7613.962787	9.165722	-0.097183	4.702058
497.547441	7621.877478	9.170727	-0.097325	4.704460
497.608456	7630.022469	9.175731	-0.097341	4.706931
497.598135	7637.979831	9.180736	-0.097344	4.709344
497.433726	7646.143378	9.185741	-0.097319	4.711818
497.630842	7654.041138	9.190746	-0.097361	4.714210
497.925539	7662.068389	9.195751	-0.097421	4.716640
498.293161	7669.994068	9.200755	-0.097494	4.719038
498.636469	7678.084838	9.205760	-0.097564	4.721484
498.843397	7686.068500	9.210765	-0.097607	4.723897
499.351374	7694.058402	9.215770	-0.097707	4.726310
499.668803	7702.042971	9.220775	-0.097771	4.728721
500.164621	7710.138577	9.225779	-0.097869	4.731163
500.151026	7718.117785	9.230784	-0.097872	4.733570
500.545262	7726.194291	9.235789	-0.097950	4.736004
500.352377	7734.260135	9.240794	-0.097919	4.738436
500.512296	7742.291426	9.245799	-0.097954	4.740854
500.329715	7750.257672	9.250803	-0.097926	4.743253
500.760659	7758.220614	9.255808	-0.098011	4.745648
500.790264	7766.327583	9.260813	-0.098022	4.748086
500.588595	7774.343192	9.265818	-0.097989	4.750496
500.973385	7782.289098	9.270823	-0.098066	4.752882
501.286508	7790.336250	9.275827	-0.098130	4.755297
501.393323	7798.314924	9.280832	-0.098155	4.757691
501.626887	7806.353019	9.285837	-0.098203	4.760102
501.680154	7814.316440	9.290842	-0.098218	4.762489
502.148515	7822.277618	9.295847	-0.098311	4.764874
502.714011	7830.346141	9.300851	-0.098421	4.767288
502.857912	7838.372870	9.305856	-0.098453	4.769691
503.643221	7846.438689	9.310861	-0.098605	4.772102
503.381581	7854.432852	9.315866	-0.098561	4.774493
503.756181	7862.475534	9.320871	-0.098636	4.776896
504.024021	7870.451188	9.325875	-0.098691	4.779278
503.807081	7878.563464	9.330880	-0.098656	4.781701
504.391677	7886.429560	9.335885	-0.098770	4.784046
504.629592	7894.482012	9.340890	-0.098819	4.786447
505.204716	7902.449422	9.345895	-0.098932	4.788821
505.218928	7910.537850	9.350899	-0.098939	4.791231
505.022390	7918.584771	9.355904	-0.098908	4.793628
505.339965	7926.647353	9.360909	-0.098972	4.796027
505.232315	7934.582734	9.365914	-0.098958	4.798389
505.334473	7942.604512	9.370919	-0.098982	4.800774
505.613069	7950.606379	9.375923	-0.099039	4.803151
506.355075	7958.543877	9.380928	-0.099182	4.805506
506.044872	7966.715304	9.385933	-0.099130	4.807934
506.739435	7974.629926	9.390938	-0.099264	4.810280
506.569136	7982.725076	9.395943	-0.099238	4.812682
507.276071	7990.128834	9.400947	-0.099374	4.814875
507.765483	7994.800053	9.405952	-0.099468	4.816257

507.577862	7997.499874	9.410957	-0.099435	4.817058
507.707941	7998.906365	9.415962	-0.099460	4.817474
507.593213	7999.357851	9.420967	-0.099439	4.817608
507.234183	8000.251620	9.425971	-0.099373	4.817875
507.940934	8000.222770	9.430976	-0.099504	4.817863
507.644808	8000.270155	9.435981	-0.099449	4.817878
507.625773	8000.267770	9.440986	-0.099445	4.817878
508.076275	8000.292152	9.445991	-0.099529	4.817883
507.997393	8000.262561	9.450995	-0.099514	4.817875
507.658003	8000.275600	9.456000	-0.099451	4.817880
507.860186	8000.333301	9.461005	-0.099489	4.817896
508.067513	8000.298336	9.466010	-0.099527	4.817885
507.808838	8000.349419	9.471015	-0.099479	4.817901
508.292998	8000.263628	9.476019	-0.099569	4.817874
508.400746	8000.280980	9.481024	-0.099589	4.817878
508.561640	8000.293827	9.486029	-0.099619	4.817881
508.450288	8000.259553	9.491034	-0.099598	4.817872
508.403916	8000.297878	9.496039	-0.099590	4.817883
507.914100	8000.399389	9.501043	-0.099499	4.817916
508.067028	8000.367858	9.506048	-0.099527	4.817906
508.422631	8000.349777	9.511053	-0.099593	4.817899
508.452528	8000.349149	9.516058	-0.099599	4.817898
508.007471	8000.372262	9.521063	-0.099516	4.817907
508.509617	8000.282513	9.526067	-0.099609	4.817878
508.689064	8000.324082	9.531072	-0.099643	4.817890
508.975457	8000.289199	9.536077	-0.099696	4.817878
508.901450	8000.289186	9.541082	-0.099682	4.817879
509.349891	8000.258739	9.546087	-0.099765	4.817868
509.676063	8000.236021	9.551091	-0.099826	4.817860
509.386360	8000.229747	9.556096	-0.099772	4.817859
509.658810	8000.271600	9.561101	-0.099823	4.817870
509.785444	8000.252338	9.566106	-0.099846	4.817864
509.461868	8000.298272	9.571111	-0.099786	4.817879
509.306078	8000.325540	9.576115	-0.099757	4.817888
509.528589	8000.308709	9.581120	-0.099798	4.817882
509.420932	8000.356693	9.586125	-0.099778	4.817896
509.323980	8000.295223	9.591130	-0.099760	4.817879
509.307663	8000.324495	9.596135	-0.099757	4.817887
509.322195	8000.342617	9.601139	-0.099760	4.817893
509.412741	8000.259601	9.606144	-0.099777	4.817868
509.299158	8000.339117	9.611149	-0.099755	4.817892
509.379199	8000.323401	9.616154	-0.099770	4.817887
509.423765	8000.368303	9.621159	-0.099779	4.817900
509.332755	8000.360668	9.626163	-0.099762	4.817898
509.516800	8000.315883	9.631168	-0.099796	4.817884
509.637965	8000.347131	9.636173	-0.099818	4.817893
510.277985	8000.237234	9.641178	-0.099937	4.817857
509.707752	8000.290162	9.646183	-0.099831	4.817876
510.516354	8000.203766	9.651187	-0.099982	4.817847
509.903203	8000.228674	9.656192	-0.099867	4.817857
509.959084	8000.319058	9.661197	-0.099878	4.817883
510.175520	8000.271577	9.666202	-0.099918	4.817868
510.193873	8000.290809	9.671207	-0.099921	4.817874
510.110171	8000.275901	9.676211	-0.099906	4.817870
509.683423	8000.307705	9.681216	-0.099826	4.817881
509.551431	8000.406981	9.686221	-0.099802	4.817911
509.891998	8000.328613	9.691226	-0.099865	4.817886
509.605379	8000.324489	9.696231	-0.099812	4.817886
509.594632	8000.364381	9.701235	-0.099810	4.817898
509.511541	8000.369506	9.706240	-0.099794	4.817900
510.213928	8000.330065	9.711245	-0.099925	4.817885
510.447779	8000.307076	9.716250	-0.099968	4.817877
511.235636	8000.204575	9.721255	-0.100115	4.817844
510.938483	8000.216107	9.726259	-0.100060	4.817848
510.718828	8000.241402	9.731264	-0.100019	4.817857
510.444360	8000.283826	9.736269	-0.099968	4.817871
510.534200	8000.237687	9.741274	-0.099984	4.817857
509.831303	8000.364590	9.746279	-0.099853	4.817897
510.135081	8000.347875	9.751283	-0.099910	4.817891
510.223695	8000.308042	9.756288	-0.099926	4.817879
510.580235	8000.306841	9.761293	-0.099993	4.817877
510.651386	8000.270973	9.766298	-0.100006	4.817866
510.351684	8000.337274	9.771303	-0.099950	4.817887
510.609940	8000.332553	9.776307	-0.099998	4.817884
510.852491	8000.233804	9.781312	-0.100043	4.817854
510.701073	8000.329641	9.786317	-0.100015	4.817883
510.526307	8000.314477	9.791322	-0.099982	4.817879
510.169354	8000.345175	9.796327	-0.099916	4.817890
510.016960	8000.390408	9.801331	-0.099887	4.817904
509.923096	8000.404864	9.806336	-0.099870	4.817909
509.972486	8000.388708	9.811341	-0.099879	4.817904
509.920325	8000.359498	9.816346	-0.099869	4.817895
510.269023	8000.323404	9.821351	-0.099934	4.817883
510.165923	8000.341944	9.826355	-0.099915	4.817889
510.497398	8000.316142	9.831360	-0.099977	4.817880
510.794396	8000.320409	9.836365	-0.100032	4.817880
510.727992	8000.303642	9.841370	-0.100019	4.817875
511.262907	8000.222799	9.846375	-0.100119	4.817849
511.014731	8000.313028	9.851379	-0.100073	4.817877
510.786782	8000.312908	9.856384	-0.100030	4.817878
510.351896	8000.379374	9.861389	-0.099949	4.817899
510.033964	8000.369529	9.866394	-0.099890	4.817898
510.629441	8000.335930	9.871399	-0.100001	4.817885
510.742827	8000.329126	9.876403	-0.100022	4.817883
510.708624	8000.333900	9.881408	-0.100015	4.817884
510.536936	8000.352507	9.886413	-0.099983	4.817891
510.384507	8000.377714	9.891418	-0.099955	4.817899
510.783301	8000.340234	9.896423	-0.100029	4.817886
511.352870	8000.313642	9.901427	-0.100135	4.817876
510.480790	8000.333769	9.906432	-0.099973	4.817885
510.817651	8000.371282	9.911437	-0.100036	4.817895
510.719930	8000.349848	9.916442	-0.100017	4.817889
510.275286	8000.404580	9.921447	-0.099934	4.817907
510.641514	8000.375062	9.926451	-0.100003	4.817897
511.023779	8000.299402	9.931456	-0.100074	4.817873
511.126059	8000.321949	9.936461	-0.100093	4.817879
511.066664	8000.278933	9.941466	-0.100082	4.817867
510.907977	8000.310374	9.946471	-0.100052	4.817876
511.127909	8000.341990	9.951475	-0.100093	4.817885
510.759259	8000.316660	9.956480	-0.100024	4.817879
510.503244	8000.356187	9.961485	-0.099977	4.817892
510.981175	8000.328276	9.966490	-0.100065	4.817881
510.680906	8000.361897	9.971495	-0.100010	4.817893
510.820676	8000.347040	9.976499	-0.100036	4.817888
510.904238	8000.313458	9.981504	-0.100051	4.817877
510.991652	8000.316819	9.986509	-0.100067	4.817878
511.084134	8000.324470	9.991514	-0.100084	4.817880
511.422187	8000.260821	9.996519	-0.100147	4.817860
511.483825	8000.278568	10.001523	-0.100159	4.817865
511.074085	8000.301128	10.006528	-0.100082	4.817873
510.997536	8000.368531	10.011533	-0.100068	4.817893
511.545527	8000.294201	10.016538	-0.100170	4.817869
511.319065	8000.318343	10.021543	-0.100128	4.817877
511.655762	8000.297888	10.026547	-0.100191	4.817870
511.665563	8000.245327	10.031552	-0.100192	4.817854
511.574822	8000.310418	10.036557	-0.100175	4.817874
511.650495	8000.285154	10.041562	-0.100189	4.817866
511.723496	8000.245096	10.046567	-0.100203	4.817854
511.768200	8000.295272	10.051571	-0.100211	4.817868
511.831942	8000.250865	10.056576	-0.100223	4.817855
511.790813	8000.288213	10.061581	-0.100215	4.817866
511.660936	8000.307420	10.066586	-0.100191	4.817872
511.816714	8000.254851	10.071591	-0.100220	4.817856
511.610787	8000.280343	10.076595	-0.100182	4.817865
511.696388	8000.233088	10.081600	-0.100198	4.817850
512.090610	8000.229270	10.086605	-0.100271	4.817847
511.898932	8000.225455	10.091610	-0.100235	4.817847
511.780347	8000.266959	10.096615	-0.100213	4.817860
512.402092	8000.228472	10.101619	-0.100329	4.817846
512.471423	8000.144093	10.106624	-0.100342	4.817821
512.334955	8000.249633	10.111629	-0.100316	4.817852
512.047124	8000.247596	10.116634	-0.100263	4.817853
512.150544	8000.229055	10.121639	-0.100282	4.817847
512.293191	8000.200538	10.126643	-0.100308	4.817838
512.023760	8000.166093	10.131648	-0.100258	4.817829
512.078863	8000.254363	10.136653	-0.100268	4.817855
511.314133	8000.307650	10.141658	-0.100126	4.817874
510.902886	8000.356537	10.146663	-0.100049	4.817890
511.095451	8000.347710	10.151667	-0.100085	4.817887
511.403924	8000.292068	10.156672	-0.100142	4.817869
511.785606	8000.293339	10.161677	-0.100214	4.817868
512.053685	8000.281383	10.166682	-0.100263	4.817863
511.593222	8000.334832	10.171687	-0.100178	4.817881
511.765950	8000.364717	10.176691	-0.100210	4.817889
511.815056	8000.265292	10.181696	-0.100219	4.817859
511.619958	8000.340476	10.186701	-0.100182	4.817882
511.463881	8000.375116	10.191706	-0.100153	4.817893
511.379257	8000.324359	10.196711	-0.100138	4.817879
511.242127	8000.349786	10.201715	-0.100112	4.817887
511.748941	8000.288565	10.206720	-0.100206	4.817867
511.421141	8000.373433	10.211725	-0.100145	4.817893
511.221465	8000.349478	10.216730	-0.100108	4.817887
511.547066	8000.340457	10.221735	-0.100169	4.817883
511.578087	8000.363033	10.226739	-0.100174	4.817889
511.772510	8000.317344	10.231744	-0.100210	4.817875
511.509963	8000.336751	10.236749	-0.100162	4.817882
511.842986	8000.333107	10.241754	-0.100224	4.817879
512.015230	8000.261803	10.246759	-0.100255	4.817857
511.765388	8000.334092	10.251763	-0.100209	4.817880
511.413448	8000.324809	10.256768	-0.100143	4.817879
511.594104	8000.380103	10.261773	-0.100177	4.817894
511.519785	8000.364275	10.266778	-0.100163	4.817890
511.166409	8000.376052	10.271783	-0.100097	4.817895
512.007118	8000.293286	10.276787	-0.100254	4.817867
511.819718	8000.294802	10.281792	-0.100219	4.817868
511.503928	8000.316605	10.286797	-0.100160	4.817876
511.780595	8000.336391	10.291802	-0.100211	4.817881
512.015043	8000.292332	10.296807	-0.100255	4.817867
511.963726	8000.306346	10.301811	-0.100245	4.817871
512.007368	8000.271135	10.306816	-0.100253	4.817860
511.613348	8000.338187	10.311821	-0.100180	4.817882
511.833223	8000.356103	10.316826	-0.100221	4.817886
511.808576	8000.325179	10.321831	-0.100216	4.817877
511.716395	8000.322796	10.326835	-0.100199	4.817877
511.702487	8000.322592	10.331840	-0.100197	4.817877
511.903371	8000.302291	10.336845	-0.100234	4.817870
511.903346	8000.347609	10.341850	-0.100234	4.817883
511.821863	8000.312706	10.346855	-0.100219	4.817873
511.335874	8000.398460	10.351859	-0.100128	4.817901
511.441681	8000.371522	10.356864	-0.100148	4.817892
511.613281	8000.439334	10.361869	-0.100180	4.817912
511.678515	8000.372814	10.366874	-0.100192	4.817892
511.672933	8000.359029	10.371879	-0.100191	4.817888
512.203882	8000.303426	10.376883	-0.100289	4.817869
512.158120	8000.257443	10.381888	-0.100281	4.817856
511.872311	8000.291271	10.386893	-0.100228	4.817867
511.882659	8000.321981	10.391898	-0.100230	4.817876
511.884584	8000.289332	10.396903	-0.100230	4.817866
512.081582	8000.331161	10.401907	-0.100267	4.817878
511.299423	8000.364171	10.406912	-0.100121	4.817891
511.745553	8000.365316	10.411917	-0.100204	4.817889
511.539575	8000.360241	10.416922	-0.100165	4.817889
511.802890	8000.332407	10.421927	-0.100214	4.817879
511.990658	8000.346699	10.426931	-0.100249	4.817883
511.923360	8000.330971	10.431936	-0.100237	4.817878
511.841783	8000.367738	10.436941	-0.100222	4.817890
512.002979	8000.354244	10.441946	-0.100252	4.817885
511.704815	8000.355220	10.446951	-0.100196	4.817886
511.600101	8000.370574	10.451955	-0.100176	4.817891
511.788145	8000.351142	10.456960	-0.100211	4.817885
511.784634	8000.374276	10.461965	-0.100211	4.817892
511.929929	8000.382687	10.466970	-0.100238	4.817894
511.797751	8000.340730	10.471975	-0.100213	4.817882
512.144357	8000.378388	10.476979	-0.100278	4.817891
511.882452	8000.364076	10.481984	-0.100229	4.817888
511.933984	8000.364814	10.486989	-0.100238	4.817888
511.996483	8000.330928	10.491994	-0.100250	4.817878
511.776626	8000.339355	10.496999	-0.100209	4.817881
511.899662	8000.360094	10.502003	-0.100232	4.817887
511.886989	8000.351476	10.507008	-0.100229	4.817885
512.059915	8000.384527	10.512013	-0.100262	4.817894
512.391775	8000.338708	10.517018	-0.100323	4.817879
512.221264	8000.305685	10.522023	-0.100291	4.817870
512.075920	8000.357343	10.527027	-0.100264	4.817886
511.863870	8000.365882	10.532032	-0.100225	4.817889
512.093525	8000.343888	10.537037	-0.100268	4.817881
511.969662	8000.366344	10.542042	-0.100244	4.817889
512.066317	8000.379325	10.547047	-0.100262	4.817892
512.189194	8000.355794	10.552051	-0.100285	4.817885
511.925635	8000.335134	10.557056	-0.100236	4.817880
512.255646	8000.368338	10.562061	-0.100298	4.817888
512.210421	8000.363467	10.567066	-0.100289	4.817887
512.253975	8000.293473	10.572071	-0.100297	4.817866
512.266914	8000.362165	10.577075	-0.100299	4.817886
512.239187	8000.313279	10.582080	-0.100294	4.817872
512.387858	8000.330171	10.587085	-0.100322	4.817876
512.553122	8000.322007	10.592090	-0.100353	4.817873
512.307533	8000.346926	10.597095	-0.100307	4.817881
512.381958	8000.363804	10.602099	-0.100321	4.817886
512.333849	8000.314625	10.607104	-0.100312	4.817872
512.712937	8000.308483	10.612109	-0.100382	4.817868
512.518942	8000.353117	10.617114	-0.100346	4.817882
512.530339	8000.338522	10.622119	-0.100348	4.817878
513.692043	8000.251950	10.627123	-0.100564	4.817847
513.912105	8000.201360	10.632128	-0.100605	4.817832
513.552436	8000.229906	10.637133	-0.100538	4.817842
513.476876	8000.179277	10.642138	-0.100524	4.817827
513.298438	8000.225189	10.647143	-0.100491	4.817841
513.699749	8000.232017	10.652147	-0.100566	4.817842
513.012434	8000.263225	10.657152	-0.100438	4.817854
512.958984	8000.287749	10.662157	-0.100428	4.817861
512.812094	8000.302495	10.667162	-0.100400	4.817866
512.846872	8000.254508	10.672167	-0.100407	4.817852
513.144950	8000.294631	10.677171	-0.100462	4.817862
513.064411	8000.289252	10.682176	-0.100447	4.817861
512.459094	8000.351154	10.687181	-0.100334	4.817882
513.013209	8000.293779	10.692186	-0.100437	4.817863
512.901700	8000.319574	10.697191	-0.100417	4.817871
512.923470	8000.365206	10.702195	-0.100421	4.817884
513.032728	8000.265591	10.707200	-0.100441	4.817854
513.855671	8000.108793	10.712205	-0.100594	4.817804
513.276781	8000.270151	10.717210	-0.100486	4.817855
513.020556	8000.234839	10.722215	-0.100438	4.817845
513.286882	8000.259750	10.727219	-0.100488	4.817852
513.124348	8000.342781	10.732224	-0.100458	4.817877
513.312926	8000.320197	10.737229	-0.100493	4.817869
513.037544	8000.279338	10.742234	-0.100441	4.817858
513.185007	8000.237190	10.747239	-0.100469	4.817845
513.235875	8000.352806	10.752243	-0.100478	4.817879
513.213851	8000.291352	10.757248	-0.100474	4.817861
513.086410	8000.317972	10.762253	-0.100450	4.817870
513.218594	8000.299846	10.767258	-0.100475	4.817864
513.007298	8000.287315	10.772263	-0.100436	4.817861
513.057028	8000.323863	10.777267	-0.100445	4.817872
513.188800	8000.288866	10.782272	-0.100469	4.817861
513.345593	8000.245798	10.787277	-0.100498	4.817847
513.267212	8000.282610	10.792282	-0.100484	4.817858
513.630479	8000.170841	10.797287	-0.100551	4.817824
513.783890	8000.285827	10.802291	-0.100580	4.817857
513.159457	8000.300021	10.807296	-0.100464	4.817864
513.737162	8000.194501	10.812301	-0.100571	4.817830
513.740968	8000.223011	10.817306	-0.100572	4.817839
513.635191	8000.287888	10.822311	-0.100552	4.817858
513.502177	8000.304942	10.827315	-0.100527	4.817864
513.818502	8000.266278	10.832320	-0.100586	4.817851
513.915949	8000.232895	10.837325	-0.100604	4.817841
513.740289	8000.233524	10.842330	-0.100571	4.817842
513.814597	8000.149216	10.847335	-0.100585	4.817817
514.010519	8000.214220	10.852339	-0.100622	4.817835
513.747243	8000.172481	10.857344	-0.100573	4.817824
513.764511	8000.127404	10.862349	-0.100576	4.817810
513.767299	8000.147467	10.867354	-0.100576	4.817816
513.495728	8000.140392	10.872359	-0.100526	4.817815
513.672560	8000.210391	10.877363	-0.100558	4.817835
513.628067	8000.250854	10.882368	-0.100550	4.817847
513.634624	8000.211946	10.887373	-0.100551	4.817836
513.326955	8000.293942	10.892378	-0.100494	4.817862
513.479669	8000.248707	10.897383	-0.100522	4.817847
513.567589	8000.272103	10.902387	-0.100539	4.817854
513.223075	8000.267140	10.907392	-0.100475	4.817854
512.702937	8000.349239	10.912397	-0.100378	4.817881
513.008592	8000.365230	10.917402	-0.100435	4.817884
512.662298	8000.329676	10.922407	-0.100370	4.817875
512.925913	8000.320819	10.927411	-0.100419	4.817871
513.011640	8000.342076	10.932416	-0.100435	4.817877
513.217793	8000.313420	10.937421	-0.100473	4.817868
513.150136	8000.310334	10.942426	-0.100461	4.817867
513.326591	8000.248577	10.947431	-0.100493	4.817848
513.111408	8000.328742	10.952435	-0.100453	4.817873
513.156118	8000.272466	10.957440	-0.100462	4.817856
513.105337	8000.283325	10.962445	-0.100452	4.817859
513.087366	8000.321008	10.967450	-0.100449	4.817871
513.616445	8000.201086	10.972455	-0.100547	4.817833
513.356028	8000.300626	10.977459	-0.100499	4.817863
513.421762	8000.285759	10.982464	-0.100511	4.817859
513.255786	8000.319202	10.987469	-0.100480	4.817869
513.134454	8000.306912	10.992474	-0.100457	4.817866
513.106739	8000.284376	10.997479	-0.100452	4.817860
513.035018	8000.364498	11.002483	-0.100439	4.817884
512.988095	8000.305849	11.007488	-0.100430	4.817867
513.334142	8000.248641	11.012493	-0.100494	4.817848
513.678283	8000.316833	11.017498	-0.100558	4.817867
513.099764	8000.342228	11.022503	-0.100451	4.817877
513.106018	8000.374989	11.027507	-0.100452	4.817886
513.173003	8000.316926	11.032512	-0.100464	4.817869
513.267690	8000.338312	11.037517	-0.100482	4.817875
512.949861	8000.373785	11.042522	-0.100423	4.817887
513.144602	8000.327047	11.047527	-0.100459	4.817872
513.050199	8000.345710	11.052531	-0.100441	4.817878
512.679968	8000.367781	11.057536	-0.100372	4.817886
512.500035	8000.436860	11.062541	-0.100339	4.817907
512.886000	8000.411847	11.067546	-0.100410	4.817898
512.985119	8000.379542	11.072551	-0.100429	4.817888
513.284463	8000.372254	11.077555	-0.100485	4.817885
513.382041	8000.271416	11.082560	-0.100503	4.817855
513.795603	8000.265773	11.087565	-0.100580	4.817851
513.435307	8000.338579	11.092570	-0.100512	4.817874
512.887909	8000.334911	11.097575	-0.100410	4.817876
513.762352	8000.344336	11.102579	-0.100573	4.817875
513.978168	8000.249416	11.107584	-0.100613	4.817846
513.803058	8000.302754	11.112589	-0.100581	4.817862
513.690571	8000.308509	11.117594	-0.100560	4.817864
513.813993	8000.278663	11.122599	-0.100583	4.817855
514.026510	8000.213208	11.127603	-0.100622	4.817835
514.061192	8000.177867	11.132608	-0.100629	4.817824
513.891983	8000.236560	11.137613	-0.100597	4.817842
514.099569	8000.277491	11.142618	-0.100636	4.817853
513.735487	8000.294379	11.147623	-0.100568	4.817860
513.883989	8000.299676	11.152627	-0.100595	4.817861
514.241705	8000.246853	11.157632	-0.100662	4.817844
513.867500	8000.266757	11.162637	-0.100592	4.817851
513.866977	8000.319448	11.167642	-0.100592	4.817867
514.092632	8000.227831	11.172647	-0.100634	4.817839
513.799801	8000.306879	11.177651	-0.100580	4.817863
513.485077	8000.308668	11.182656	-0.100521	4.817865
513.775329	8000.279115	11.187661	-0.100575	4.817855
513.551167	8000.334909	11.192666	-0.100533	4.817873
513.586229	8000.265845	11.197671	-0.100540	4.817852
514.055768	8000.210416	11.202675	-0.100627	4.817834
513.814520	8000.222749	11.207680	-0.100582	4.817838
513.177068	8000.318969	11.212685	-0.100463	4.817870
513.707079	8000.277058	11.217690	-0.100562	4.817855
514.266574	8000.209222	11.222695	-0.100666	4.817832
513.864181	8000.303556	11.227699	-0.100591	4.817862
514.186801	8000.262875	11.232704	-0.100651	4.817849
514.057302	8000.218846	11.237709	-0.100627	4.817836
513.595937	8000.335519	11.242714	-0.100541	4.817873
513.460871	8000.325139	11.247719	-0.100516	4.817870
513.636504	8000.363501	11.252723	-0.100549	4.817881
513.288936	8000.377465	11.257728	-0.100484	4.817886
513.486877	8000.329719	11.262733	-0.100521	4.817872
513.619280	8000.353757	11.267738	-0.100545	4.817878
513.449512	8000.362903	11.272743	-0.100514	4.817881
513.888192	8000.321786	11.277747	-0.100595	4.817867
513.445762	8000.328059	11.282752	-0.100513	4.817871
513.344716	8000.358222	11.287757	-0.100494	4.817881
513.672124	8000.341852	11.292762	-0.100555	4.817874
513.833525	8000.314661	11.297767	-0.100585	4.817866
513.942628	8000.334147	11.302771	-0.100605	4.817871
513.435589	8000.356354	11.307776	-0.100511	4.817880
513.223437	8000.363836	11.312781	-0.100471	4.817883
513.706613	8000.349710	11.317786	-0.100561	4.817876
513.626946	8000.334857	11.322791	-0.100546	4.817872
513.527847	8000.377695	11.327795	-0.100528	4.817886
513.542601	8000.347338	11.332800	-0.100530	4.817876
513.584459	8000.357423	11.337805	-0.100538	4.817879
513.482702	8000.381251	11.342810	-0.100519	4.817887
513.155885	8000.350192	11.347815	-0.100458	4.817879
513.560113	8000.331766	11.352819	-0.100533	4.817872
514.031360	8000.297442	11.357824	-0.100621	4.817860
514.287205	8000.263178	11.362829	-0.100669	4.817848
513.879395	8000.333192	11.367834	-0.100593	4.817871
513.546443	8000.303097	11.372839	-0.100531	4.817863
513.456591	8000.323934	11.377843	-0.100514	4.817870
513.476397	8000.362161	11.382848	-0.100518	4.817881
514.119221	8000.289200	11.387853	-0.100637	4.817857
514.083302	8000.335057	11.392858	-0.100630	4.817871
513.587980	8000.333190	11.397863	-0.100538	4.817872
513.926975	8000.344393	11.402867	-0.100601	4.817874
513.846812	8000.351667	11.407872	-0.100586	4.817876
513.596427	8000.339626	11.412877	-0.100540	4.817874
513.620133	8000.326262	11.417882	-0.100544	4.817870
513.738034	8000.346928	11.422887	-0.100566	4.817876
513.927478	8000.346491	11.427891	-0.100601	4.817875
513.066402	8000.366763	11.432896	-0.100441	4.817884
513.137833	8000.385706	11.437901	-0.100454	4.817890
513.740501	8000.378571	11.442906	-0.100566	4.817885
513.658554	8000.356307	11.447911	-0.100551	4.817879
513.690571	8000.378899	11.452915	-0.100557	4.817885
513.733220	8000.342619	11.457920	-0.100565	4.817874
514.043015	8000.298592	11.462925	-0.100622	4.817860
513.862076	8000.325495	11.467930	-0.100589	4.817869
514.129208	8000.299826	11.472935	-0.100638	4.817860
514.019019	8000.307722	11.477939	-0.100618	4.817863
514.116985	8000.275401	11.482944	-0.100636	4.817853
513.761424	8000.282925	11.487949	-0.100570	4.817857
513.751152	8000.321773	11.492954	-0.100568	4.817868
513.634314	8000.297952	11.497959	-0.100546	4.817862
513.961181	8000.301602	11.502963	-0.100607	4.817861
514.263612	8000.280657	11.507968	-0.100663	4.817854
514.840879	8000.195160	11.512973	-0.100770	4.817826
514.691647	8000.235168	11.517978	-0.100743	4.817838
514.428988	8000.241922	11.522983	-0.100694	4.817842
514.435301	8000.257820	11.527987	-0.100695	4.817846
514.653311	8000.254632	11.532992	-0.100735	4.817844
514.087419	8000.220128	11.537997	-0.100630	4.817837
514.754524	8000.216030	11.543002	-0.100754	4.817832
514.149350	8000.296903	11.548007	-0.100641	4.817859
513.901413	8000.363949	11.553011	-0.100595	4.817880
513.968017	8000.324851	11.558016	-0.100608	4.817868
513.746466	8000.353278	11.563021	-0.100566	4.817877
513.706922	8000.356921	11.568026	-0.100559	4.817879
513.713810	8000.343315	11.573031	-0.100560	4.817875
513.615697	8000.418842	11.578035	-0.100542	4.817897
514.072987	8000.345318	11.583040	-0.100627	4.817874
513.625097	8000.369431	11.588045	-0.100543	4.817883
513.646633	8000.362360	11.593050	-0.100547	4.817881
514.142418	8000.293607	11.598055	-0.100640	4.817858
514.109485	8000.324750	11.603059	-0.100633	4.817867
514.043815	8000.322746	11.608064	-0.100621	4.817867
514.003225	8000.281051	11.613069	-0.100614	4.817855
513.849777	8000.357890	11.618074	-0.100585	4.817878
514.116087	8000.282670	11.623079	-0.100634	4.817855
514.359340	8000.297764	11.628083	-0.100680	4.817858
513.687892	8000.376629	11.633088	-0.100555	4.817885
513.908781	8000.314457	11.638093	-0.100596	4.817865
513.888895	8000.375301	11.643098	-0.100592	4.817883
514.308167	8000.325473	11.648103	-0.100670	4.817867
514.412981	8000.282709	11.653107	-0.100689	4.817854
514.585539	8000.271489	11.658112	-0.100722	4.817850
514.641539	8000.253320	11.663117	-0.100732	4.817844
514.757548	8000.305581	11.668122	-0.100754	4.817859
514.370264	8000.274702	11.673127	-0.100681	4.817852
514.394721	8000.316158	11.678131	-0.100686	4.817864
514.201662	8000.302834	11.683136	-0.100650	4.817861
514.142236	8000.313569	11.688141	-0.100639	4.817864
514.348765	8000.327081	11.693146	-0.100677	4.817867
514.279725	8000.284975	11.698151	-0.100664	4.817855
514.152267	8000.346378	11.703155	-0.100641	4.817874
514.108495	8000.345744	11.708160	-0.100632	4.817874
514.470251	8000.261358	11.713165	-0.100700	4.817847
514.174888	8000.300316	11.718170	-0.100645	4.817860
514.030992	8000.252917	11.723175	-0.100618	4.817847
514.448707	8000.288443	11.728179	-0.100695	4.817855
514.216639	8000.312501	11.733184	-0.100652	4.817863
514.076663	8000.297834	11.738189	-0.100626	4.817860
513.763379	8000.367100	11.743194	-0.100568	4.817881
514.540437	8000.221238	11.748199	-0.100712	4.817835
514.475434	8000.238217	11.753203	-0.100700	4.817840
514.455126	8000.300109	11.758208	-0.100696	4.817859
514.952180	8000.168132	11.763213	-0.100789	4.817817
514.966121	8000.205221	11.768218	-0.100791	4.817828
514.663511	8000.204021	11.773223	-0.100735	4.817829
514.882384	8000.178711	11.778227	-0.100776	4.817821
514.885723	8000.220917	11.783232	-0.100776	4.817833
514.720678	8000.153186	11.788237	-0.100746	4.817814
514.617671	8000.249724	11.793242	-0.100726	4.817843
514.946207	8000.195427	11.798247	-0.100787	4.817826
514.814213	8000.250441	11.803251	-0.100763	4.817842
514.757398	8000.233808	11.808256	-0.100752	4.817838
514.849822	8000.213001	11.813261	-0.100769	4.817831
514.506425	8000.322942	11.818266	-0.100705	4.817865
514.751990	8000.231612	11.823271	-0.100751	4.817837
514.600437	8000.275803	11.828275	-0.100723	4.817851
514.674856	8000.309547	11.833280	-0.100737	4.817861
514.284805	8000.320789	11.838285	-0.100664	4.817866
514.433337	8000.332412	11.843290	-0.100692	4.817868
514.234551	8000.293708	11.848295	-0.100655	4.817858
514.089664	8000.334833	11.853299	-0.100628	4.817871
513.892654	8000.342532	11.858304	-0.100591	4.817874
514.029965	8000.311832	11.863309	-0.100616	4.817864
514.730047	8000.287129	11.868314	-0.100747	4.817854
514.383513	8000.305323	11.873319	-0.100682	4.817861
514.284857	8000.296520	11.878323	-0.100664	4.817858
514.256468	8000.271865	11.883328	-0.100658	4.817851
514.506319	8000.198515	11.888333	-0.100705	4.817828
514.223082	8000.320917	11.893338	-0.100652	4.817866
513.756025	8000.372158	11.898343	-0.100565	4.817883
513.992440	8000.365019	11.903347	-0.100609	4.817880
513.878874	8000.349678	11.908352	-0.100588	4.817876
513.983970	8000.331161	11.913357	-0.100607	4.817870
514.503543	8000.277508	11.918362	-0.100704	4.817852
514.065944	8000.295444	11.923367	-0.100622	4.817859
514.084099	8000.326269	11.928371	-0.100626	4.817868
514.440018	8000.337717	11.933376	-0.100692	4.817870
514.224817	8000.348316	11.938381	-0.100652	4.817874
514.063410	8000.378662	11.943386	-0.100622	4.817884
514.361898	8000.316554	11.948391	-0.100677	4.817864
514.073129	8000.357715	11.953395	-0.100624	4.817877
514.323690	8000.336024	11.958400	-0.100670	4.817870
514.669762	8000.256682	11.963405	-0.100735	4.817845
514.842681	8000.366683	11.968410	-0.100767	4.817877
514.898076	8000.296856	11.973415	-0.100777	4.817856
515.012730	8000.272153	11.978419	-0.100798	4.817848
514.530401	8000.285228	11.983424	-0.100708	4.817854
514.421611	8000.282604	11.988429	-0.100688	4.817854
514.342617	8000.315192	11.993434	-0.100673	4.817864
514.547425	8000.266490	11.998439	-0.100711	4.817848
514.577497	8000.320676	12.003443	-0.100717	4.817864
514.398449	8000.301229	12.008448	-0.100684	4.817859
514.290909	8000.285974	12.013453	-0.100664	4.817855
514.664771	8000.260789	12.018458	-0.100733	4.817846
514.589730	8000.256542	12.023463	-0.100719	4.817845
514.630873	8000.261348	12.028467	-0.100727	4.817847
514.788613	8000.292076	12.033472	-0.100756	4.817855
515.007287	8000.248845	12.038477	-0.100797	4.817841
514.862483	8000.296295	12.043482	-0.100770	4.817856
515.080148	8000.286779	12.048487	-0.100810	4.817852
514.901488	8000.306337	12.053491	-0.100777	4.817859
514.509873	8000.330205	12.058496	-0.100704	4.817867
514.297881	8000.307121	12.063501	-0.100664	4.817862
514.429771	8000.327990	12.068506	-0.100689	4.817867
514.205193	8000.293131	12.073511	-0.100647	4.817858
514.530256	8000.317836	12.078515	-0.100708	4.817864
514.348326	8000.358428	12.083520	-0.100674	4.817876
514.287746	8000.339633	12.088525	-0.100662	4.817871
514.270898	8000.371008	12.093530	-0.100659	4.817881
514.308599	8000.326224	12.098535	-0.100666	4.817867
514.458592	8000.354732	12.103539	-0.100694	4.817875
514.401127	8000.313847	12.108544	-0.100683	4.817863
513.801377	8000.342097	12.113549	-0.100572	4.817874
513.839373	8000.407990	12.118554	-0.100579	4.817893
514.082440	8000.371435	12.123559	-0.100624	4.817881
514.054483	8000.373137	12.128563	-0.100619	4.817882
513.921218	8000.372268	12.133568	-0.100594	4.817882
513.689374	8000.392114	12.138573	-0.100551	4.817889
513.502317	8000.430524	12.143578	-0.100516	4.817901
513.426388	8000.395698	12.148583	-0.100501	4.817891
513.549115	8000.444893	12.153587	-0.100524	4.817906
513.776109	8000.419700	12.158592	-0.100567	4.817897
513.328271	8000.354222	12.163597	-0.100483	4.817880
513.895695	8000.401389	12.168602	-0.100589	4.817891
514.089920	8000.367292	12.173607	-0.100625	4.817880
514.000720	8000.411327	12.178611	-0.100608	4.817894
513.737028	8000.413850	12.183616	-0.100559	4.817896
513.719085	8000.413588	12.188621	-0.100556	4.817896
513.814962	8000.424452	12.193626	-0.100573	4.817898
513.453236	8000.411861	12.198631	-0.100506	4.817896
513.450677	8000.447657	12.203635	-0.100506	4.817907
513.447522	8000.473959	12.208640	-0.100505	4.817915
513.450531	8000.430784	12.213645	-0.100505	4.817902
513.758809	8000.431004	12.218650	-0.100563	4.817901
513.970809	8000.378191	12.223655	-0.100602	4.817884
514.042287	8000.414000	12.228659	-0.100615	4.817894
514.164339	8000.371485	12.233664	-0.100638	4.817881
513.892931	8000.407625	12.238669	-0.100588	4.817893
513.736349	8000.451744	12.243674	-0.100558	4.817907
514.041125	8000.404483	12.248679	-0.100615	4.817891
514.006463	8000.435601	12.253683	-0.100609	4.817901
514.589277	8000.352292	12.258688	-0.100717	4.817874
514.113418	8000.343326	12.263693	-0.100628	4.817873
514.545317	8000.368517	12.268698	-0.100709	4.817879
514.178779	8000.383260	12.273703	-0.100640	4.817885
514.030942	8000.413802	12.278707	-0.100613	4.817894
513.806098	8000.379993	12.283712	-0.100571	4.817885
513.665748	8000.442264	12.288717	-0.100545	4.817904
514.306755	8000.409333	12.293722	-0.100664	4.817892
514.019696	8000.366195	12.298727	-0.100611	4.817880
514.624796	8000.352773	12.303731	-0.100723	4.817874
514.611323	8000.363116	12.308736	-0.100721	4.817877
514.470902	8000.355819	12.313741	-0.100694	4.817875
514.255793	8000.414906	12.318746	-0.100654	4.817894
514.075626	8000.400712	12.323751	-0.100621	4.817890
514.201528	8000.410955	12.328755	-0.100644	4.817893
514.416517	8000.387698	12.333760	-0.100684	4.817885
514.319844	8000.351518	12.338765	-0.100666	4.817875
514.629127	8000.333835	12.343770	-0.100724	4.817868
514.530664	8000.359818	12.348775	-0.100705	4.817876
514.746196	8000.360812	12.353779	-0.100745	4.817876
514.986472	8000.328433	12.358784	-0.100790	4.817865
514.426270	8000.375169	12.363789	-0.100686	4.817881
514.799203	8000.345755	12.368794	-0.100755	4.817871
514.841631	8000.297876	12.373799	-0.100763	4.817857
514.598360	8000.349179	12.378803	-0.100718	4.817873
514.289632	8000.374241	12.383808	-0.100660	4.817881
514.494226	8000.371915	12.388813	-0.100698	4.817880
514.551825	8000.390660	12.393818	-0.100709	4.817885
514.110674	8000.390625	12.398823	-0.100627	4.817887
514.327135	8000.395848	12.403827	-0.100667	4.817888
514.443929	8000.358528	12.408832	-0.100689	4.817876
514.908156	8000.249267	12.413837	-0.100775	4.817842
514.605577	8000.358742	12.418842	-0.100719	4.817876
514.593933	8000.340652	12.423847	-0.100716	4.817870
514.427837	8000.378309	12.428851	-0.100685	4.817882
514.336800	8000.348535	12.433856	-0.100668	4.817874
514.333579	8000.333729	12.438861	-0.100668	4.817869
514.299357	8000.403853	12.443866	-0.100661	4.817890
514.832041	8000.316660	12.448871	-0.100760	4.817862
515.229454	8000.284436	12.453875	-0.100834	4.817851
514.696171	8000.349479	12.458880	-0.100735	4.817872
514.198160	8000.397111	12.463885	-0.100642	4.817889
514.458119	8000.399799	12.468890	-0.100691	4.817888
514.689639	8000.384158	12.473895	-0.100734	4.817883
514.842493	8000.388465	12.478899	-0.100762	4.817883
514.849786	8000.379080	12.483904	-0.100764	4.817881
515.130544	8000.277717	12.488909	-0.100816	4.817849
515.251624	8000.333215	12.493914	-0.100838	4.817865
515.279239	8000.280907	12.498919	-0.100843	4.817850
515.818749	8000.189596	12.503923	-0.100944	4.817820
515.673990	8000.239156	12.508928	-0.100917	4.817836
515.471783	8000.189860	12.513933	-0.100879	4.817822
515.731442	8000.263166	12.518938	-0.100927	4.817842
515.801159	8000.203032	12.523943	-0.100940	4.817824
515.935498	8000.168072	12.528947	-0.100965	4.817813
515.881225	8000.173611	12.533952	-0.100955	4.817815
515.807356	8000.253706	12.538957	-0.100941	4.817839
515.782853	8000.256511	12.543962	-0.100937	4.817840
515.613615	8000.248799	12.548967	-0.100905	4.817839
515.678477	8000.228649	12.553971	-0.100917	4.817832
515.331093	8000.324829	12.558976	-0.100852	4.817862
515.325198	8000.250957	12.563981	-0.100851	4.817841
515.254891	8000.316346	12.568986	-0.100838	4.817860
515.064866	8000.289361	12.573991	-0.100803	4.817853
515.714630	8000.224936	12.578995	-0.100924	4.817831
515.488977	8000.257519	12.584000	-0.100882	4.817842
515.303088	8000.246405	12.589005	-0.100847	4.817839
515.190171	8000.330153	12.594010	-0.100826	4.817865
515.073014	8000.352704	12.599015	-0.100804	4.817872
515.163390	8000.303409	12.604019	-0.100821	4.817857
515.499775	8000.327226	12.609024	-0.100883	4.817862
515.144776	8000.293647	12.614029	-0.100817	4.817854
515.259671	8000.364867	12.619034	-0.100839	4.817875
514.904823	8000.348156	12.624039	-0.100773	4.817871
514.717458	8000.354939	12.629043	-0.100738	4.817874
514.370931	8000.371024	12.634048	-0.100673	4.817880
514.461123	8000.314348	12.639053	-0.100690	4.817863
514.934788	8000.352790	12.644058	-0.100778	4.817872
514.833873	8000.375576	12.649063	-0.100759	4.817880
514.698317	8000.355700	12.654067	-0.100734	4.817874
514.843398	8000.350409	12.659072	-0.100761	4.817872
514.986366	8000.290276	12.664077	-0.100787	4.817854
514.809891	8000.374162	12.669082	-0.100754	4.817879
515.052782	8000.328118	12.674087	-0.100800	4.817865
514.929578	8000.356907	12.679091	-0.100777	4.817874
514.862618	8000.379128	12.684096	-0.100764	4.817881
514.611087	8000.275366	12.689101	-0.100717	4.817851
515.036329	8000.331029	12.694106	-0.100796	4.817866
514.982819	8000.328147	12.699111	-0.100786	4.817865
515.115671	8000.283679	12.704115	-0.100811	4.817851
515.220096	8000.307316	12.709120	-0.100830	4.817858
514.956950	8000.303521	12.714125	-0.100781	4.817858
515.147517	8000.311533	12.719130	-0.100817	4.817859
515.048705	8000.317484	12.724135	-0.100798	4.817862
515.297078	8000.322114	12.729139	-0.100845	4.817862
515.526476	8000.313822	12.734144	-0.100887	4.817858
515.278307	8000.252269	12.739149	-0.100841	4.817841
515.553661	8000.302612	12.744154	-0.100892	4.817855
515.468938	8000.280306	12.749159	-0.100876	4.817849
515.646036	8000.214341	12.754163	-0.100909	4.817828
515.136883	8000.316623	12.759168	-0.100814	4.817861
515.294469	8000.271458	12.764173	-0.100844	4.817847
514.964865	8000.347867	12.769178	-0.100782	4.817871
515.473423	8000.207624	12.774183	-0.100877	4.817827
515.663479	8000.181899	12.779187	-0.100912	4.817819
515.584558	8000.268246	12.784192	-0.100898	4.817845
515.588737	8000.265140	12.789197	-0.100898	4.817844
515.601966	8000.281139	12.794202	-0.100901	4.817848
515.494933	8000.240592	12.799207	-0.100881	4.817837
515.042654	8000.351072	12.804211	-0.100797	4.817872
515.197046	8000.335374	12.809216	-0.100825	4.817866
515.251652	8000.296104	12.814221	-0.100835	4.817854
515.336655	8000.344758	12.819226	-0.100851	4.817868
515.243716	8000.304415	12.824231	-0.100834	4.817857
515.065139	8000.330298	12.829235	-0.100801	4.817865
515.162954	8000.341190	12.834240	-0.100819	4.817868
515.023469	8000.336015	12.839245	-0.100793	4.817867
515.123819	8000.371187	12.844250	-0.100811	4.817877
515.151552	8000.359989	12.849255	-0.100816	4.817874
515.562599	8000.264719	12.854259	-0.100893	4.817844
515.495986	8000.337540	12.859264	-0.100880	4.817866
515.631235	8000.237242	12.864269	-0.100906	4.817835
515.884950	8000.272517	12.869274	-0.100953	4.817845
515.705709	8000.278362	12.874279	-0.100919	4.817847
515.395657	8000.307621	12.879283	-0.100862	4.817857
515.676080	8000.316929	12.884288	-0.100914	4.817859
515.555873	8000.267760	12.889293	-0.100891	4.817845
515.861882	8000.257410	12.894298	-0.100948	4.817840
515.583276	8000.329284	12.899303	-0.100896	4.817863
515.405665	8000.303532	12.904307	-0.100863	4.817856
515.539242	8000.291750	12.909312	-0.100888	4.817852
515.360018	8000.262813	12.914317	-0.100855	4.817844
515.961723	8000.171344	12.919322	-0.100967	4.817814
515.842848	8000.175952	12.924327	-0.100944	4.817816
516.088662	8000.133112	12.929331	-0.100990	4.817803
516.118937	8000.204168	12.934336	-0.100996	4.817823
516.113567	8000.159816	12.939341	-0.100995	4.817810
516.027648	8000.254495	12.944346	-0.100979	4.817839
515.986464	8000.232816	12.949351	-0.100971	4.817832
515.804111	8000.259698	12.954355	-0.100937	4.817841
516.049452	8000.187338	12.959360	-0.100983	4.817819
515.813173	8000.201848	12.964365	-0.100939	4.817824
516.120101	8000.153565	12.969370	-0.100996	4.817808
516.253304	8000.158644	12.974375	-0.101020	4.817809
515.904170	8000.201041	12.979379	-0.100955	4.817823
516.179027	8000.258757	12.984384	-0.101007	4.817839
516.061918	8000.192767	12.989389	-0.100985	4.817820
516.076037	8000.254104	12.994394	-0.100987	4.817838
515.982934	8000.230623	12.999399	-0.100970	4.817832
516.048567	8000.154618	13.004403	-0.100982	4.817809
515.981937	8000.262224	13.009408	-0.100970	4.817841
515.982594	8000.247473	13.014413	-0.100970	4.817837
516.190082	8000.211459	13.019418	-0.101008	4.817825
515.546693	8000.267535	13.024423	-0.100888	4.817845
515.578171	8000.294337	13.029427	-0.100894	4.817852
515.609625	8000.358031	13.034432	-0.100900	4.817871
514.943967	8000.384272	13.039437	-0.100776	4.817882
515.238098	8000.384291	13.044442	-0.100831	4.817881
515.949216	8000.275428	13.049447	-0.100963	4.817845
516.152453	8000.241461	13.054451	-0.101001	4.817834
515.647880	8000.337484	13.059456	-0.100907	4.817865
515.335786	8000.336145	13.064461	-0.100849	4.817866
515.990357	8000.305521	13.069466	-0.100971	4.817854
515.840139	8000.252757	13.074471	-0.100943	4.817839
516.123078	8000.202020	13.079475	-0.100995	4.817823
516.096207	8000.222710	13.084480	-0.100990	4.817829
515.736321	8000.193277	13.089485	-0.100923	4.817822
516.003592	8000.172881	13.094490	-0.100973	4.817815
516.298241	8000.204531	13.099495	-0.101028	4.817823
515.802210	8000.255352	13.104499	-0.100935	4.817840
515.843956	8000.267545	13.109504	-0.100943	4.817843
516.012077	8000.206720	13.114509	-0.100974	4.817825
515.954406	8000.299698	13.119514	-0.100964	4.817852
516.267923	8000.165076	13.124519	-0.101022	4.817811
516.270898	8000.116628	13.129523	-0.101022	4.817797
516.112764	8000.245050	13.134528	-0.100993	4.817836
515.671858	8000.279801	13.139533	-0.100911	4.817848
515.709163	8000.318281	13.144538	-0.100918	4.817859
515.865047	8000.295227	13.149543	-0.100947	4.817852
515.728644	8000.262690	13.154547	-0.100921	4.817842
516.005097	8000.268779	13.159552	-0.100973	4.817843
515.617725	8000.277949	13.164557	-0.100900	4.817847
516.085728	8000.257285	13.169562	-0.100987	4.817839
515.854050	8000.304538	13.174567	-0.100944	4.817854
515.646351	8000.297325	13.179571	-0.100906	4.817853
515.302966	8000.344022	13.184576	-0.100842	4.817868
515.754894	8000.290450	13.189581	-0.100926	4.817851
515.592571	8000.328161	13.194586	-0.100895	4.817862
515.672706	8000.330367	13.199591	-0.100910	4.817863
515.627495	8000.306522	13.204595	-0.100902	4.817856
515.375362	8000.359805	13.209600	-0.100855	4.817873
515.984695	8000.274772	13.214605	-0.100968	4.817845
516.077906	8000.283490	13.219610	-0.100986	4.817847
515.898359	8000.301980	13.224615	-0.100952	4.817853
515.590319	8000.295429	13.229619	-0.100895	4.817853
515.711395	8000.337225	13.234624	-0.100917	4.817865
515.668823	8000.248066	13.239629	-0.100909	4.817838
515.768457	8000.277959	13.244634	-0.100928	4.817847
516.269350	8000.201903	13.249639	-0.101021	4.817822
516.205789	8000.166199	13.254643	-0.101009	4.817812
515.829991	8000.296754	13.259648	-0.100939	4.817852
515.929738	8000.174863	13.264653	-0.100958	4.817816
516.053440	8000.259914	13.269658	-0.100981	4.817840
515.947786	8000.259441	13.274663	-0.100961	4.817841
515.920440	8000.281179	13.279667	-0.100956	4.817847
516.285912	8000.257984	13.284672	-0.101024	4.817839
516.312066	8000.174031	13.289677	-0.101029	4.817814
516.218106	8000.215891	13.294682	-0.101011	4.817827
516.159464	8000.211880	13.299687	-0.101000	4.817826
516.293503	8000.232782	13.304691	-0.101025	4.817831
516.533087	8000.218313	13.309696	-0.101070	4.817826
515.798904	8000.286782	13.314701	-0.100933	4.817849
516.242556	8000.277362	13.319706	-0.101015	4.817845
516.014417	8000.286719	13.324711	-0.100973	4.817848
516.294707	8000.184294	13.329715	-0.101025	4.817817
515.935259	8000.299274	13.334720	-0.100958	4.817852
515.941214	8000.192896	13.339725	-0.100959	4.817821
516.107047	8000.261689	13.344730	-0.100990	4.817841
516.131659	8000.169282	13.349735	-0.100994	4.817813
516.347269	8000.148142	13.354739	-0.101034	4.817806
516.092813	8000.236176	13.359744	-0.100987	4.817833
515.959066	8000.178379	13.364749	-0.100962	4.817817
516.144918	8000.261163	13.369754	-0.100997	4.817840
516.333270	8000.198522	13.374759	-0.101032	4.817821
516.447017	8000.148509	13.379763	-0.101053	4.817806
516.436454	8000.135704	13.384768	-0.101051	4.817802
516.767751	8000.130990	13.389773	-0.101112	4.817799
516.505605	8000.155667	13.394778	-0.101064	4.817807
516.530000	8000.140204	13.399783	-0.101068	4.817803
516.481528	8000.150043	13.404787	-0.101059	4.817806
516.710727	8000.138586	13.409792	-0.101102	4.817802
516.380276	8000.127495	13.414797	-0.101040	4.817800
516.366018	8000.152584	13.419802	-0.101037	4.817807
516.455925	8000.237149	13.424807	-0.101054	4.817832
516.437913	8000.196831	13.429811	-0.101051	4.817820
516.054901	8000.277741	13.434816	-0.100979	4.817846
516.406351	8000.203747	13.439821	-0.101045	4.817822
516.590918	8000.264379	13.444826	-0.101079	4.817839
516.443811	8000.295986	13.449831	-0.101052	4.817849
516.186149	8000.237456	13.454835	-0.101004	4.817833
516.148751	8000.346537	13.459840	-0.100997	4.817866
515.911080	8000.279863	13.464845	-0.100952	4.817847
516.010326	8000.316075	13.469850	-0.100971	4.817857
516.252225	8000.254206	13.474855	-0.101016	4.817838
516.088121	8000.246566	13.479859	-0.100985	4.817836
516.330933	8000.253225	13.484864	-0.101030	4.817837
516.102941	8000.280503	13.489869	-0.100988	4.817846
515.760457	8000.324051	13.494874	-0.100924	4.817861
515.927210	8000.309586	13.499879	-0.100955	4.817856
515.978295	8000.273426	13.504883	-0.100965	4.817845
516.323583	8000.313185	13.509888	-0.101029	4.817855
515.840423	8000.294621	13.514893	-0.100939	4.817852
515.781858	8000.328558	13.519898	-0.100928	4.817862
516.059770	8000.276695	13.524903	-0.100980	4.817845
516.020177	8000.249769	13.529907	-0.100972	4.817837
516.013393	8000.309750	13.534912	-0.100971	4.817855
515.569309	8000.324427	13.539917	-0.100888	4.817862
515.791159	8000.331837	13.544922	-0.100929	4.817863
515.731609	8000.333084	13.549927	-0.100918	4.817863
516.319935	8000.246694	13.554931	-0.101028	4.817835
516.526830	8000.320297	13.559936	-0.101066	4.817856
515.973975	8000.243809	13.564941	-0.100963	4.817836
515.913815	8000.269290	13.569946	-0.100952	4.817844
515.615473	8000.366177	13.574951	-0.100896	4.817874
516.138515	8000.249332	13.579955	-0.100994	4.817837
516.126425	8000.313453	13.584960	-0.100991	4.817856
516.014900	8000.313950	13.589965	-0.100971	4.817857
515.889976	8000.310038	13.594970	-0.100947	4.817856
516.079774	8000.268499	13.599975	-0.100983	4.817843
515.871589	8000.280252	13.604979	-0.100944	4.817847
515.496298	8000.370760	13.609984	-0.100874	4.817876
515.371186	8000.345764	13.614989	-0.100851	4.817869
515.606181	8000.370228	13.619994	-0.100894	4.817875
516.270884	8000.318670	13.624999	-0.101018	4.817857
516.151898	8000.280059	13.630003	-0.100996	4.817846
515.979224	8000.326054	13.635008	-0.100964	4.817860
516.108472	8000.278372	13.640013	-0.100988	4.817846
516.403620	8000.332165	13.645018	-0.101043	4.817860
516.173936	8000.348878	13.650023	-0.101000	4.817866
515.713897	8000.341189	13.655027	-0.100914	4.817866
516.164021	8000.368756	13.660032	-0.100998	4.817872
515.700006	8000.344144	13.665037	-0.100911	4.817867
515.440149	8000.403639	13.670042	-0.100863	4.817886
515.496791	8000.441345	13.675047	-0.100873	4.817896
515.815411	8000.345797	13.680051	-0.100933	4.817867
515.705867	8000.378999	13.685056	-0.100912	4.817877
515.423253	8000.383355	13.690061	-0.100860	4.817880
515.525439	8000.387986	13.695066	-0.100879	4.817881
515.365022	8000.375130	13.700071	-0.100849	4.817877
515.959263	8000.245608	13.705075	-0.100959	4.817837
516.001605	8000.342136	13.710080	-0.100967	4.817865
515.808628	8000.320378	13.715085	-0.100931	4.817859
515.448862	8000.376325	13.720090	-0.100864	4.817877
515.639702	8000.366423	13.725095	-0.100900	4.817874
515.400139	8000.420941	13.730099	-0.100855	4.817891
515.612351	8000.397644	13.735104	-0.100894	4.817883
515.410346	8000.335701	13.740109	-0.100857	4.817866
515.042053	8000.417878	13.745114	-0.100788	4.817891
515.267012	8000.405305	13.750119	-0.100830	4.817887
515.557317	8000.375756	13.755123	-0.100884	4.817877
515.817497	8000.375286	13.760128	-0.100932	4.817876
515.596814	8000.349966	13.765133	-0.100891	4.817869
515.781850	8000.351576	13.770138	-0.100926	4.817869
515.688394	8000.369199	13.775143	-0.100908	4.817874
515.686509	8000.347033	13.780147	-0.100908	4.817868
516.062412	8000.352448	13.785152	-0.100978	4.817868
516.588095	8000.274643	13.790157	-0.101076	4.817842
515.970252	8000.337409	13.795162	-0.100961	4.817864
516.019465	8000.357089	13.800167	-0.100970	4.817869
515.726935	8000.334949	13.805171	-0.100915	4.817864
516.233435	8000.348572	13.810176	-0.101009	4.817866
515.972065	8000.316340	13.815181	-0.100961	4.817857
515.935976	8000.246248	13.820186	-0.100954	4.817837
516.177072	8000.308748	13.825191	-0.100999	4.817854
515.755268	8000.350098	13.830195	-0.100920	4.817868
516.002811	8000.307283	13.835200	-0.100966	4.817855
515.765263	8000.310180	13.840205	-0.100922	4.817857
515.759894	8000.355424	13.845210	-0.100921	4.817870
515.865279	8000.344291	13.850215	-0.100940	4.817866
515.786296	8000.313635	13.855219	-0.100926	4.817857
516.136871	8000.339767	13.860224	-0.100991	4.817864
516.302780	8000.282073	13.865229	-0.101022	4.817846
516.111938	8000.354158	13.870234	-0.100986	4.817868
516.164798	8000.349646	13.875239	-0.100996	4.817867
516.127621	8000.305889	13.880243	-0.100989	4.817854
516.014780	8000.352747	13.885248	-0.100968	4.817868
515.597731	8000.367813	13.890253	-0.100890	4.817874
515.628950	8000.378800	13.895258	-0.100896	4.817877
515.537690	8000.382752	13.900263	-0.100879	4.817879
515.227610	8000.389874	13.905267	-0.100821	4.817882
515.383302	8000.406871	13.910272	-0.100850	4.817887
515.886156	8000.324520	13.915277	-0.100944	4.817860
515.610809	8000.393279	13.920282	-0.100893	4.817882
515.383890	8000.413194	13.925287	-0.100850	4.817889
515.559533	8000.358802	13.930291	-0.100883	4.817872
515.846360	8000.379799	13.935296	-0.100936	4.817877
516.007716	8000.350499	13.940301	-0.100966	4.817867
515.606777	8000.418501	13.945306	-0.100892	4.817889
515.710100	8000.397851	13.950311	-0.100911	4.817883
515.274675	8000.408437	13.955315	-0.100830	4.817888
515.656196	8000.410771	13.960320	-0.100901	4.817887
515.388409	8000.415340	13.965325	-0.100851	4.817889
515.458897	8000.434271	13.970330	-0.100864	4.817895
515.305304	8000.447865	13.975335	-0.100835	4.817899
515.382918	8000.406818	13.980339	-0.100850	4.817887
514.982405	8000.457961	13.985344	-0.100775	4.817904
514.388438	8000.495777	13.990349	-0.100664	4.817917
515.415163	8000.395677	13.995354	-0.100855	4.817883
515.327167	8000.424974	14.000359	-0.100839	4.817892
514.883581	8000.447037	14.005363	-0.100756	4.817901
515.128773	8000.387323	14.010368	-0.100802	4.817882
515.220079	8000.371771	14.015373	-0.100819	4.817877
515.208558	8000.438007	14.020378	-0.100817	4.817897
515.523083	8000.389834	14.025383	-0.100875	4.817881
515.387539	8000.396309	14.030387	-0.100850	4.817884
515.538037	8000.430097	14.035392	-0.100878	4.817893
515.556189	8000.401895	14.040397	-0.100881	4.817885
515.297256	8000.451917	14.045402	-0.100833	4.817901
515.684468	8000.370007	14.050407	-0.100905	4.817875
515.867361	8000.339964	14.055411	-0.100939	4.817865
515.481987	8000.407137	14.060416	-0.100867	4.817886
515.549462	8000.418647	14.065421	-0.100880	4.817890
515.638396	8000.407276	14.070426	-0.100896	4.817886
515.676371	8000.374090	14.075431	-0.100903	4.817876
515.981823	8000.298380	14.080435	-0.100960	4.817852
515.907755	8000.375310	14.085440	-0.100946	4.817875
515.401154	8000.392248	14.090445	-0.100852	4.817882
515.218951	8000.435998	14.095450	-0.100818	4.817896
514.916414	8000.398958	14.100455	-0.100762	4.817886
515.373887	8000.407656	14.105459	-0.100847	4.817887
515.888749	8000.382398	14.110464	-0.100943	4.817877
515.665407	8000.383391	14.115469	-0.100901	4.817879
515.455375	8000.414090	14.120474	-0.100862	4.817889
515.459642	8000.370932	14.125479	-0.100863	4.817876
515.498382	8000.373595	14.130483	-0.100870	4.817876
515.771687	8000.365936	14.135488	-0.100921	4.817873
515.473646	8000.376393	14.140493	-0.100865	4.817877
515.355143	8000.409466	14.145498	-0.100843	4.817888
515.450693	8000.393975	14.150503	-0.100861	4.817883
515.373321	8000.411830	14.155507	-0.100846	4.817888
515.570120	8000.420987	14.160512	-0.100883	4.817890
515.441550	8000.395941	14.165517	-0.100859	4.817883
515.452669	8000.430882	14.170522	-0.100861	4.817894
515.668583	8000.412910	14.175527	-0.100901	4.817887
515.660533	8000.370627	14.180531	-0.100899	4.817875
515.700514	8000.408093	14.185536	-0.100907	4.817886
515.230417	8000.429773	14.190541	-0.100819	4.817894
515.215858	8000.435884	14.195546	-0.100817	4.817896
515.528411	8000.397169	14.200551	-0.100875	4.817883
515.383566	8000.381375	14.205555	-0.100848	4.817879
515.612418	8000.394157	14.210560	-0.100890	4.817882
514.981373	8000.471491	14.215565	-0.100773	4.817908
515.144233	8000.446429	14.220570	-0.100803	4.817900
515.256115	8000.360551	14.225575	-0.100824	4.817874
515.390263	8000.395157	14.230579	-0.100849	4.817883
515.612303	8000.393084	14.235584	-0.100890	4.817882
514.965219	8000.426971	14.240589	-0.100769	4.817895
515.203099	8000.435666	14.245594	-0.100814	4.817896
515.197038	8000.423981	14.250599	-0.100813	4.817893
515.394805	8000.350935	14.255603	-0.100849	4.817870
514.918590	8000.249205	14.260608	-0.100760	4.817842
515.225173	8000.419105	14.265613	-0.100818	4.817891
515.287870	8000.448465	14.270618	-0.100829	4.817900
515.331506	8000.370036	14.275623	-0.100837	4.817876
515.056173	8000.359740	14.280627	-0.100786	4.817874
515.109721	8000.398455	14.285632	-0.100796	4.817886
515.338801	8000.405969	14.290637	-0.100839	4.817887
515.274746	8000.421907	14.295642	-0.100827	4.817892
515.045841	8000.395416	14.300647	-0.100784	4.817885
515.548302	8000.395275	14.305651	-0.100877	4.817883
515.839093	8000.361517	14.310656	-0.100932	4.817872
515.653494	8000.357784	14.315661	-0.100897	4.817871
515.675953	8000.401321	14.320666	-0.100901	4.817884
515.277704	8000.464092	14.325671	-0.100827	4.817904
515.261968	8000.417483	14.330675	-0.100824	4.817891
515.744132	8000.392807	14.335680	-0.100914	4.817881
516.079860	8000.319642	14.340685	-0.100976	4.817858
515.862201	8000.358664	14.345690	-0.100936	4.817871
515.614253	8000.428871	14.350695	-0.100889	4.817892
515.829343	8000.331831	14.355699	-0.100929	4.817863
516.049661	8000.387708	14.360704	-0.100970	4.817878
516.054058	8000.337172	14.365709	-0.100971	4.817863
516.074256	8000.353271	14.370714	-0.100975	4.817868
515.791692	8000.388195	14.375719	-0.100922	4.817880
515.808792	8000.346275	14.380723	-0.100925	4.817867
515.884633	8000.392690	14.385728	-0.100939	4.817881
516.100153	8000.367333	14.390733	-0.100979	4.817872
516.421770	8000.313992	14.395738	-0.101039	4.817855
516.159209	8000.352367	14.400743	-0.100990	4.817867
516.081694	8000.336489	14.405747	-0.100976	4.817863
516.026909	7999.410242	14.410752	-0.100965	4.817589

515.981532	7996.140356	14.415757	-0.100954	4.816621
516.221792	7990.633302	14.420762	-0.100995	4.814988
515.982149	7984.064051	14.425767	-0.100947	4.813041
515.588499	7976.779664	14.430771	-0.100868	4.810883
515.355348	7969.178958	14.435776	-0.100820	4.808629
515.579131	7961.313614	14.440781	-0.100857	4.806293
515.354308	7953.369339	14.445786	-0.100809	4.803935
515.369844	7945.600281	14.450791	-0.100807	4.801626
515.290235	7937.514542	14.455795	-0.100787	4.799223
515.480931	7929.566455	14.460800	-0.100817	4.796859
515.654313	7921.475156	14.465805	-0.100844	4.794450
515.503809	7913.599852	14.470810	-0.100811	4.792106
515.239648	7905.517511	14.475815	-0.100757	4.789700
514.756721	7897.587556	14.480819	-0.100662	4.787338
515.419292	7889.462627	14.485824	-0.100780	4.784913
515.287994	7881.593997	14.490829	-0.100750	4.782567
515.809649	7873.489883	14.495834	-0.100842	4.780146
515.676242	7865.520358	14.500839	-0.100812	4.777767
515.657937	7857.479857	14.505843	-0.100803	4.775365
515.530932	7849.537273	14.510848	-0.100774	4.772991
515.353992	7841.505280	14.515853	-0.100736	4.770590
515.722958	7833.447600	14.520858	-0.100799	4.768178
515.655488	7825.471793	14.525863	-0.100781	4.765790
515.858509	7817.445400	14.530867	-0.100814	4.763386
515.755512	7809.544989	14.535872	-0.100790	4.761019
515.958638	7801.503658	14.540877	-0.100822	4.758607
515.653962	7793.514629	14.545882	-0.100760	4.756212
515.624167	7785.478201	14.550887	-0.100749	4.753800
515.710363	7777.536311	14.555891	-0.100760	4.751415
515.572706	7769.463424	14.560896	-0.100729	4.748990
515.104642	7761.493641	14.565901	-0.100637	4.746596
515.420514	7753.425692	14.570906	-0.100690	4.744169
515.396834	7745.513532	14.575911	-0.100681	4.741788
515.355563	7737.447622	14.580915	-0.100668	4.739360
515.660368	7729.502579	14.585920	-0.100719	4.736967
515.396481	7721.431762	14.590925	-0.100665	4.734535
514.903235	7713.471159	14.595930	-0.100568	4.732136
514.937485	7705.475161	14.600935	-0.100569	4.729724
515.175070	7697.453649	14.605939	-0.100608	4.727303
514.920660	7689.459659	14.610944	-0.100555	4.724890
514.590281	7681.508612	14.615949	-0.100488	4.722488
515.066103	7673.430667	14.620954	-0.100572	4.720045
515.213784	7665.481611	14.625959	-0.100594	4.717641
514.572915	7657.512154	14.630963	-0.100469	4.715231
514.070218	7649.527223	14.635968	-0.100371	4.712815
514.240794	7641.474175	14.640973	-0.100397	4.710375
514.349807	7633.465070	14.645978	-0.100412	4.707948
514.212782	7625.481401	14.650983	-0.100381	4.705527
514.573140	7617.383043	14.655987	-0.100443	4.703070
514.240840	7609.486928	14.660992	-0.100376	4.700674
514.163504	7601.425567	14.665997	-0.100356	4.698226
514.188593	7593.457254	14.671002	-0.100356	4.695805
514.051472	7585.470785	14.676007	-0.100325	4.693377
514.421392	7577.395177	14.681011	-0.100389	4.690920
514.019636	7569.447795	14.686016	-0.100309	4.688502
514.219451	7561.439281	14.691021	-0.100341	4.686064
514.213093	7553.443353	14.696026	-0.100334	4.683628
514.166244	7545.473988	14.701031	-0.100320	4.681199
513.981951	7537.417256	14.706035	-0.100281	4.678742
514.034662	7529.521036	14.711040	-0.100285	4.676333
513.372315	7521.505208	14.716045	-0.100157	4.673887
512.898704	7513.458567	14.721050	-0.100063	4.671429
512.985137	7505.418715	14.726055	-0.100074	4.668972
513.176884	7497.409843	14.731059	-0.100104	4.666523
513.237531	7489.327307	14.736064	-0.100110	4.664051
513.632406	7481.427082	14.741069	-0.100179	4.661632
513.394613	7473.430923	14.746074	-0.100129	4.659184
513.281578	7465.494255	14.751079	-0.100103	4.656752
512.953691	7457.430182	14.756083	-0.100036	4.654280
513.108217	7449.456506	14.761088	-0.100060	4.651834
512.730939	7441.402110	14.766093	-0.099984	4.649363
512.671837	7433.430628	14.771098	-0.099968	4.646915
513.077855	7425.400599	14.776103	-0.100039	4.644448
512.867362	7417.419207	14.781107	-0.099994	4.641995
512.554618	7409.414716	14.786112	-0.099931	4.639533
512.550714	7401.466294	14.791117	-0.099925	4.637087
512.246212	7393.412684	14.796122	-0.099863	4.634608
512.116491	7385.467784	14.801127	-0.099833	4.632160
512.030425	7377.340774	14.806131	-0.099812	4.629656
512.140940	7369.426528	14.811136	-0.099827	4.627215
511.642111	7361.429086	14.816141	-0.099729	4.624748
512.136711	7353.375170	14.821146	-0.099816	4.622261
512.327028	7345.400638	14.826151	-0.099846	4.619799
512.265781	7337.383247	14.831155	-0.099829	4.617321
512.123077	7329.375392	14.836160	-0.099798	4.614845
512.485360	7321.370852	14.841165	-0.099860	4.612369
512.172099	7313.424445	14.846170	-0.099796	4.609909
512.517357	7305.358842	14.851175	-0.099855	4.607411
512.670807	7297.243602	14.856179	-0.099879	4.604897
511.973686	7289.492559	14.861184	-0.099744	4.602493
511.926392	7281.395719	14.866189	-0.099730	4.599982
511.854333	7273.353692	14.871194	-0.099711	4.597486
512.048442	7265.388526	14.876199	-0.099742	4.595012
511.737769	7257.406308	14.881203	-0.099679	4.592532
511.623090	7249.355495	14.886208	-0.099652	4.590029
511.607614	7241.359904	14.891213	-0.099644	4.587542
511.553403	7233.248479	14.896218	-0.099628	4.585018
511.523625	7225.417090	14.901223	-0.099618	4.582579
510.999502	7217.370763	14.906227	-0.099515	4.580071
511.140802	7209.373924	14.911232	-0.099536	4.577579
511.135310	7201.325087	14.916237	-0.099530	4.575068
511.146001	7193.323602	14.921242	-0.099526	4.572571
510.903207	7185.363840	14.926247	-0.099476	4.570086
511.089690	7177.347176	14.931251	-0.099505	4.567581
510.869917	7169.307231	14.936256	-0.099459	4.565068
510.539873	7161.380247	14.941261	-0.099392	4.562588
510.553833	7153.342884	14.946266	-0.099390	4.560073
511.030566	7145.333934	14.951271	-0.099473	4.557566
510.954685	7137.276039	14.956275	-0.099454	4.555042
510.985147	7129.329475	14.961280	-0.099454	4.552551
510.835783	7121.292963	14.966285	-0.099421	4.550031
510.560439	7113.276789	14.971290	-0.099365	4.547514
510.534016	7105.295157	14.976295	-0.099355	4.545008
510.427720	7097.334443	14.981299	-0.099329	4.542507
510.439928	7089.348452	14.986304	-0.099327	4.539997
510.525920	7081.270031	14.991309	-0.099337	4.537457
510.444970	7073.223251	14.996314	-0.099317	4.534925
510.345532	7065.309040	15.001319	-0.099293	4.532433
509.984139	7057.266707	15.006323	-0.099221	4.529898
510.213093	7049.271429	15.011328	-0.099258	4.527379
509.896583	7041.310105	15.016333	-0.099194	4.524867
509.851545	7033.287568	15.021338	-0.099180	4.522336
509.998270	7025.312257	15.026343	-0.099202	4.519818
509.874229	7017.286598	15.031347	-0.099174	4.517282
509.627109	7009.275579	15.036352	-0.099123	4.514749
509.724578	7001.316097	15.041357	-0.099135	4.512232
509.618720	6993.200324	15.046362	-0.099110	4.509664
509.691843	6985.295390	15.051367	-0.099119	4.507161
509.608496	6977.155080	15.056371	-0.099098	4.504582
509.809672	6969.251782	15.061376	-0.099130	4.502078
510.113540	6961.200146	15.066381	-0.099182	4.499525
509.525084	6953.270988	15.071386	-0.099067	4.497007
509.400775	6945.246941	15.076391	-0.099038	4.494459
509.417045	6937.268143	15.081395	-0.099036	4.491924
509.115887	6929.217020	15.086400	-0.098975	4.489364
509.545116	6921.202236	15.091405	-0.099049	4.486816
509.396468	6913.186021	15.096410	-0.099016	4.484265
509.721911	6905.257859	15.101415	-0.099072	4.481741
509.216892	6897.187576	15.106419	-0.098972	4.479168
509.629038	6889.218308	15.111424	-0.099044	4.476629
509.569531	6881.197780	15.116429	-0.099028	4.474071
509.382035	6873.217758	15.121434	-0.098987	4.471523
508.998807	6865.231258	15.126439	-0.098911	4.468971
509.332842	6857.168597	15.131443	-0.098968	4.466397
509.363097	6849.161436	15.136448	-0.098968	4.463837
509.192878	6841.260164	15.141453	-0.098931	4.461309
508.793414	6833.196964	15.146458	-0.098852	4.458726
509.391582	6825.238539	15.151463	-0.098958	4.456180
509.206266	6817.144675	15.156467	-0.098918	4.453586
509.311169	6809.172108	15.161472	-0.098932	4.451030
509.392591	6801.186920	15.166477	-0.098942	4.448469
509.006348	6793.163685	15.171482	-0.098865	4.445892
509.285782	6785.146877	15.176487	-0.098912	4.443318
509.127051	6777.226777	15.181491	-0.098877	4.440772
508.978078	6769.198543	15.186496	-0.098844	4.438190
508.862529	6761.201687	15.191501	-0.098817	4.435617
508.986192	6753.138834	15.196506	-0.098835	4.433022
509.307040	6745.146289	15.201511	-0.098889	4.430449
509.104158	6737.100932	15.206515	-0.098846	4.427855
508.955236	6729.103043	15.211520	-0.098813	4.425275
508.829511	6721.153992	15.216525	-0.098785	4.422709
509.051739	6713.104185	15.221530	-0.098821	4.420111
508.810530	6705.185756	15.226535	-0.098771	4.417552
508.974459	6697.100897	15.231539	-0.098796	4.414939
509.135808	6689.153978	15.236544	-0.098821	4.412370
508.812737	6681.166158	15.241549	-0.098755	4.409783
508.250169	6673.175863	15.246554	-0.098645	4.407192
508.580566	6665.089652	15.251559	-0.098701	4.404574
507.937825	6657.235705	15.256563	-0.098577	4.402024
507.714080	6649.223000	15.261568	-0.098530	4.399424
507.956998	6641.219916	15.266573	-0.098570	4.396827
508.333222	6633.079624	15.271578	-0.098634	4.394186
508.024054	6625.191433	15.276583	-0.098572	4.391620
507.947805	6617.103869	15.281587	-0.098552	4.388990
507.957814	6609.162451	15.286592	-0.098549	4.386406
508.127421	6601.101799	15.291597	-0.098575	4.383783
508.076484	6593.147998	15.296602	-0.098560	4.381192
507.945603	6585.189992	15.301607	-0.098531	4.378597
508.066490	6577.157047	15.306611	-0.098548	4.375978
507.966662	6569.129534	15.311616	-0.098524	4.373358
507.885867	6561.158105	15.316621	-0.098504	4.370754
507.999773	6553.098592	15.321626	-0.098520	4.368122
508.314562	6545.085522	15.326631	-0.098573	4.365505
508.253480	6537.110837	15.331635	-0.098556	4.362895
508.240381	6529.184749	15.336640	-0.098549	4.360301
508.021643	6521.238270	15.341645	-0.098503	4.357697
507.454651	6513.254667	15.346650	-0.098392	4.355077
507.633437	6505.251215	15.351655	-0.098420	4.352454
508.062911	6497.121424	15.356659	-0.098495	4.349789
507.698865	6489.178591	15.361664	-0.098422	4.347179
507.353794	6481.173750	15.366669	-0.098352	4.344547
507.164110	6473.234952	15.371674	-0.098312	4.341936
507.260367	6465.173014	15.376679	-0.098324	4.339285
507.067181	6457.216530	15.381683	-0.098283	4.336665
507.240530	6449.194814	15.386688	-0.098310	4.334025
507.081728	6441.250120	15.391693	-0.098275	4.331406
506.849732	6433.199387	15.396698	-0.098227	4.328749
507.246039	6425.174671	15.401703	-0.098295	4.326105
506.907186	6417.204520	15.406707	-0.098227	4.323471
506.547188	6409.272952	15.411712	-0.098155	4.320849
506.807513	6401.221669	15.416717	-0.098198	4.318190
506.593829	6393.238818	15.421722	-0.098153	4.315548
506.929286	6385.188855	15.426727	-0.098210	4.312887
506.809875	6377.142851	15.431731	-0.098182	4.310221
506.819429	6369.196594	15.436736	-0.098179	4.307589
506.824704	6361.140460	15.441741	-0.098175	4.304918
506.566375	6353.188273	15.446746	-0.098121	4.302277
506.519171	6345.140676	15.451751	-0.098107	4.299606
506.380934	6337.188797	15.456755	-0.098076	4.296963
506.204857	6329.149899	15.461760	-0.098038	4.294290
505.920702	6321.240934	15.466765	-0.097980	4.291657
505.730687	6313.157188	15.471770	-0.097939	4.288965
506.118099	6305.188751	15.476775	-0.098006	4.286315
506.119737	6297.109032	15.481779	-0.098001	4.283623
505.973377	6289.217214	15.486784	-0.097969	4.280991
506.033512	6281.190892	15.491789	-0.097975	4.278314
505.813271	6273.195058	15.496794	-0.097929	4.275642
505.909214	6265.192751	15.501799	-0.097941	4.272970
506.064006	6257.098532	15.506803	-0.097965	4.270266
505.852531	6249.142859	15.511808	-0.097920	4.267604
505.761697	6241.135673	15.516813	-0.097898	4.264923
505.914645	6233.134075	15.521818	-0.097921	4.262245
505.667146	6225.156391	15.526823	-0.097870	4.259569
505.505183	6217.186943	15.531827	-0.097834	4.256896
505.549602	6209.174714	15.536832	-0.097837	4.254208
505.694648	6201.155296	15.541837	-0.097859	4.251517
505.751305	6193.074757	15.546842	-0.097864	4.248803
505.804493	6185.132241	15.551847	-0.097869	4.246134
505.603190	6177.144774	15.556851	-0.097826	4.243445
505.707815	6169.131938	15.561856	-0.097841	4.240749
505.854843	6161.159949	15.566861	-0.097863	4.238066
505.536268	6153.159896	15.571866	-0.097798	4.235367
505.647409	6145.141738	15.576871	-0.097814	4.232664
505.356875	6137.153994	15.581875	-0.097754	4.229966
505.564199	6129.095949	15.586880	-0.097788	4.227247
505.698602	6121.078542	15.591885	-0.097807	4.224540
505.365745	6113.176909	15.596890	-0.097740	4.221865
505.182850	6105.169595	15.601895	-0.097701	4.219154
505.336196	6097.143911	15.606899	-0.097724	4.216439
505.483220	6089.113410	15.611904	-0.097746	4.213720
505.523136	6081.130158	15.616909	-0.097748	4.211014
505.158629	6073.124635	15.621914	-0.097675	4.208295
505.636527	6065.097005	15.626919	-0.097759	4.205576
505.394278	6057.116354	15.631923	-0.097709	4.202863
505.144556	6049.175190	15.636928	-0.097657	4.200161
505.123550	6041.187608	15.641933	-0.097648	4.197445
505.176150	6033.113791	15.646938	-0.097652	4.194698
504.889812	6025.154693	15.651943	-0.097594	4.191985
505.221218	6017.019733	15.656947	-0.097650	4.189217
505.006119	6009.066928	15.661952	-0.097605	4.186503
504.683928	6001.126688	15.666957	-0.097540	4.183790
505.396520	5993.066635	15.671962	-0.097667	4.181047
505.000326	5985.132078	15.676967	-0.097588	4.178332
504.683336	5977.158101	15.681971	-0.097524	4.175602
504.432439	5969.163447	15.686976	-0.097472	4.172864
504.456662	5961.128024	15.691981	-0.097471	4.170114
504.414591	5953.081104	15.696986	-0.097458	4.167358
504.710959	5945.016597	15.701991	-0.097508	4.164597
504.363902	5937.175016	15.706995	-0.097438	4.161903
504.332361	5929.113636	15.712000	-0.097427	4.159136
504.177864	5921.226565	15.717005	-0.097393	4.156426
503.925346	5913.155731	15.722010	-0.097340	4.153649
504.469341	5905.121267	15.727015	-0.097436	4.150893
504.373363	5897.101773	15.732019	-0.097413	4.148132
504.313038	5889.075476	15.737024	-0.097397	4.145368
504.335032	5881.152961	15.742029	-0.097396	4.142638
504.090004	5873.127937	15.747034	-0.097345	4.139868
504.270818	5865.173866	15.752039	-0.097373	4.137126
504.425581	5857.087677	15.757043	-0.097397	4.134336
504.471397	5849.155544	15.762048	-0.097400	4.131596
504.204322	5841.142154	15.767053	-0.097345	4.128822
504.149897	5833.166740	15.772058	-0.097330	4.126063
504.230362	5825.125702	15.777063	-0.097339	4.123280
503.937343	5817.189164	15.782067	-0.097280	4.120527
504.023590	5809.187532	15.787072	-0.097290	4.117754
503.696087	5801.253272	15.792077	-0.097224	4.114997
504.243976	5793.094181	15.797082	-0.097321	4.112172
503.699243	5785.173065	15.802087	-0.097214	4.109413
503.877583	5777.147191	15.807091	-0.097242	4.106626
503.948025	5769.110353	15.812096	-0.097250	4.103832
503.400002	5761.230996	15.817101	-0.097143	4.101081
503.553789	5753.109460	15.822106	-0.097166	4.098255
503.666225	5745.155416	15.827111	-0.097182	4.095484
503.377945	5737.167480	15.832115	-0.097123	4.092694
503.607640	5729.079970	15.837120	-0.097160	4.089874
503.439069	5721.201896	15.842125	-0.097124	4.087121
503.354852	5713.100713	15.847130	-0.097103	4.084288
503.129633	5705.239458	15.852135	-0.097056	4.081535
502.864778	5697.175693	15.857139	-0.097001	4.078709
503.026820	5689.225483	15.862144	-0.097026	4.075927
502.988534	5681.190185	15.867149	-0.097014	4.073111
503.048952	5673.127839	15.872154	-0.097020	4.070284
502.833869	5665.200108	15.877159	-0.096974	4.067498
502.601703	5657.138222	15.882163	-0.096926	4.064664
502.957123	5649.133364	15.887168	-0.096987	4.061856
502.911957	5641.117349	15.892173	-0.096973	4.059036
502.888324	5633.161872	15.897178	-0.096963	4.056236
502.832087	5625.165461	15.902183	-0.096948	4.053419
502.278152	5617.178551	15.907187	-0.096839	4.050596
502.633407	5609.131224	15.912192	-0.096900	4.047763
502.560375	5601.142651	15.917197	-0.096881	4.044943
502.448882	5593.184357	15.922202	-0.096855	4.042130
502.981352	5585.104275	15.927207	-0.096949	4.039283
502.577500	5577.246870	15.932211	-0.096869	4.036498
502.400638	5569.162711	15.937216	-0.096830	4.033634
502.111904	5561.169579	15.942221	-0.096771	4.030799
502.360647	5553.089328	15.947226	-0.096812	4.027939
501.985498	5545.144990	15.952231	-0.096737	4.025115
502.314824	5537.125175	15.957235	-0.096793	4.022274
502.959702	5529.025335	15.962240	-0.096908	4.019408
502.421644	5521.173070	15.967245	-0.096803	4.016609
502.490103	5513.133665	15.972250	-0.096810	4.013750
502.487640	5505.162865	15.977255	-0.096805	4.010913
502.821331	5497.108526	15.982259	-0.096861	4.008050
502.518621	5489.171740	15.987264	-0.096800	4.005216
502.555010	5481.208231	15.992269	-0.096801	4.002377
502.242849	5473.202021	15.997274	-0.096738	3.999514
502.148260	5465.294531	16.002279	-0.096715	3.996688
502.278569	5457.189078	16.007283	-0.096734	3.993793
502.252663	5449.224260	16.012288	-0.096724	3.990943
502.234917	5441.218551	16.017293	-0.096716	3.988077
502.036390	5433.156702	16.022298	-0.096673	3.985186
502.076927	5425.235556	16.027303	-0.096676	3.982347
501.991433	5417.214779	16.032307	-0.096654	3.979468
501.615347	5409.283485	16.037312	-0.096579	3.976614
501.491348	5401.260646	16.042317	-0.096551	3.973730
501.115946	5393.269001	16.047322	-0.096476	3.970850
501.258132	5385.228428	16.052327	-0.096497	3.967960
500.978532	5377.200571	16.057331	-0.096439	3.965065
501.554667	5369.190082	16.062336	-0.096542	3.962189
501.601756	5361.178550	16.067341	-0.096545	3.959301
501.478978	5353.240998	16.072346	-0.096517	3.956434
501.212772	5345.263712	16.077351	-0.096462	3.953549
501.523265	5337.190853	16.082355	-0.096515	3.950637
501.040559	5329.227684	16.087360	-0.096420	3.947749
501.158438	5321.200482	16.092365	-0.096436	3.944846
501.012913	5313.220107	16.097370	-0.096404	3.941953
500.706771	5305.260742	16.102375	-0.096342	3.939063
500.367472	5297.283239	16.107379	-0.096273	3.936163
500.991983	5289.178824	16.112384	-0.096384	3.933233
500.845184	5281.203324	16.117389	-0.096352	3.930334
501.308562	5273.102588	16.122394	-0.096433	3.927398
501.310901	5265.151793	16.127399	-0.096428	3.924505
500.850269	5257.289315	16.132403	-0.096337	3.921634
500.821757	5249.245691	16.137408	-0.096326	3.918703
500.728020	5241.319389	16.142413	-0.096304	3.915812
500.567762	5233.281892	16.147418	-0.096268	3.912876
500.679318	5225.249785	16.152423	-0.096284	3.909946
500.364981	5217.281311	16.157427	-0.096220	3.907028
500.726128	5209.182195	16.162432	-0.096282	3.904073
500.750573	5201.292997	16.167437	-0.096281	3.901187
500.221573	5193.292797	16.172442	-0.096178	3.898246
500.287207	5185.297458	16.177447	-0.096185	3.895317
500.024550	5177.324176	16.182451	-0.096130	3.892387
500.168598	5169.245655	16.187456	-0.096152	3.889425
500.197324	5161.285716	16.192461	-0.096152	3.886502
500.209262	5153.227412	16.197466	-0.096149	3.883539
500.203698	5145.289040	16.202471	-0.096143	3.880619
499.960626	5137.334135	16.207475	-0.096092	3.877685
500.027861	5129.285203	16.212480	-0.096100	3.874721
499.724610	5121.233340	16.217485	-0.096038	3.871745
499.845539	5113.158270	16.222490	-0.096055	3.868768
500.004009	5105.165862	16.227495	-0.096079	3.865820
500.127022	5097.184011	16.232499	-0.096097	3.862872
500.256010	5089.216308	16.237504	-0.096116	3.859928
500.039171	5081.326428	16.242509	-0.096070	3.857003
500.395944	5073.189420	16.247514	-0.096131	3.853996
500.198086	5065.310688	16.252519	-0.096089	3.851071
500.464696	5057.200416	16.257523	-0.096133	3.848068
499.984387	5049.271064	16.262528	-0.096039	3.845113
500.280761	5041.324425	16.267533	-0.096089	3.842167
500.027421	5033.264370	16.272538	-0.096036	3.839164
500.547038	5025.293521	16.277543	-0.096128	3.836209
499.880684	5017.344585	16.282547	-0.095999	3.833234
499.938680	5009.315594	16.287552	-0.096004	3.830242
499.573540	5001.371103	16.292557	-0.095931	3.827271
499.397262	4993.284790	16.297562	-0.095893	3.824248
500.078318	4985.312435	16.302567	-0.096014	3.821284
499.805902	4977.342938	16.307571	-0.095958	3.818298
499.573192	4969.346594	16.312576	-0.095910	3.815301
499.217002	4961.449802	16.317581	-0.095838	3.812336
499.005094	4953.378364	16.322586	-0.095793	3.809306
498.806021	4945.412518	16.327591	-0.095751	3.806313
498.999261	4937.306480	16.332595	-0.095782	3.803275
498.942174	4929.358123	16.337600	-0.095766	3.800287
498.602858	4921.415643	16.342605	-0.095698	3.797293
498.608481	4913.335134	16.347610	-0.095693	3.794253
499.152557	4905.307139	16.352615	-0.095789	3.791242
498.618397	4897.359243	16.357619	-0.095685	3.788234
498.700700	4889.286740	16.362624	-0.095695	3.785191
498.735748	4881.392243	16.367629	-0.095696	3.782212
499.014060	4873.276706	16.372634	-0.095743	3.779152
498.566290	4865.422058	16.377639	-0.095654	3.776172
498.642896	4857.375596	16.382643	-0.095663	3.773129
498.752122	4849.365712	16.387648	-0.095678	3.770098
498.692429	4841.383450	16.392653	-0.095662	3.767071
498.808039	4833.316060	16.397658	-0.095678	3.764014
498.354994	4825.486457	16.402663	-0.095588	3.761031
498.494821	4817.386162	16.407667	-0.095609	3.757957
498.545123	4809.399853	16.412672	-0.095613	3.754921
498.562307	4801.444223	16.417677	-0.095611	3.751894
498.702076	4793.375799	16.422682	-0.095632	3.748824
499.003665	4785.331471	16.427687	-0.095683	3.745765
498.557371	4777.444388	16.432691	-0.095594	3.742746
498.404106	4769.444576	16.437696	-0.095561	3.739688
498.642944	4761.454793	16.442701	-0.095600	3.736641
498.023025	4753.487558	16.447706	-0.095479	3.733579
497.861299	4745.539944	16.452711	-0.095444	3.730533
497.445896	4737.539566	16.457715	-0.095361	3.727458
497.421864	4729.458682	16.462720	-0.095352	3.724359
497.724922	4721.503931	16.467725	-0.095403	3.721315
497.607419	4713.451400	16.472730	-0.095376	3.718220
497.476256	4705.484480	16.477735	-0.095346	3.715154
497.548880	4697.437780	16.482739	-0.095354	3.712061
497.676271	4689.387664	16.487744	-0.095373	3.708965
497.740771	4681.431806	16.492749	-0.095379	3.705902
497.503786	4673.444234	16.497754	-0.095330	3.702816
497.303452	4665.494149	16.502759	-0.095287	3.699742
497.337520	4657.505229	16.507763	-0.095289	3.696658
497.193340	4649.484846	16.512768	-0.095256	3.693553
497.668792	4641.437756	16.517773	-0.095340	3.690452
497.408000	4633.455646	16.522778	-0.095286	3.687355
497.285057	4625.445292	16.527783	-0.095258	3.684247
497.091908	4617.553516	16.532787	-0.095217	3.681181
497.214306	4609.492639	16.537792	-0.095234	3.678055
497.287310	4601.517431	16.542797	-0.095242	3.674958
497.102658	4593.503111	16.547802	-0.095203	3.671837
497.280115	4585.490145	16.552807	-0.095230	3.668723
496.986918	4577.529846	16.557811	-0.095171	3.665614
496.559982	4569.576040	16.562816	-0.095086	3.662502
496.840433	4561.553151	16.567821	-0.095133	3.659379
497.010945	4553.533418	16.572826	-0.095159	3.656252
497.093110	4545.515433	16.577831	-0.095169	3.653120
497.454012	4537.456166	16.582835	-0.095231	3.649977
497.114658	4529.554603	16.587840	-0.095163	3.646874
496.920743	4521.597179	16.592845	-0.095122	3.643751
496.793045	4513.598259	16.597850	-0.095093	3.640610
496.805075	4505.648141	16.602855	-0.095090	3.637489
497.031305	4497.577727	16.607859	-0.095126	3.634325
496.432815	4489.655962	16.612864	-0.095010	3.631193
496.313055	4481.649437	16.617869	-0.094982	3.628039
496.394252	4473.593642	16.622874	-0.094992	3.624868
496.679181	4465.608685	16.627879	-0.095040	3.621728
497.231122	4457.519684	16.632883	-0.095137	3.618551
497.002847	4449.603365	16.637888	-0.095090	3.615418
496.782079	4441.668214	16.642893	-0.095043	3.612275
496.540853	4433.605092	16.647898	-0.094993	3.609079
496.358123	4425.670301	16.652903	-0.094954	3.605931
496.504487	4417.648576	16.657907	-0.094976	3.602756
496.756483	4409.582125	16.662912	-0.095017	3.599564
496.853100	4401.671602	16.667917	-0.095030	3.596426
496.570013	4393.651999	16.672922	-0.094972	3.593231
496.745973	4385.662499	16.677927	-0.095000	3.590058
496.705700	4377.655903	16.682931	-0.094987	3.586870
496.146753	4369.693896	16.687936	-0.094878	3.583681
496.326013	4361.734763	16.692941	-0.094906	3.580512
496.071573	4353.749063	16.697946	-0.094853	3.577317
496.453644	4345.689747	16.702951	-0.094919	3.574108
496.489381	4337.703096	16.707955	-0.094920	3.570916
496.179886	4329.698674	16.712960	-0.094858	3.567703
496.086909	4321.719676	16.717965	-0.094835	3.564504
495.648285	4313.811970	16.722970	-0.094748	3.561320
495.874730	4305.769734	16.727975	-0.094785	3.558099
496.060544	4297.749402	16.732979	-0.094814	3.554883
496.086036	4289.680847	16.737984	-0.094814	3.551640
495.661378	4281.764687	16.742989	-0.094729	3.548442
495.158967	4273.772678	16.747994	-0.094631	3.545207
495.310147	4265.797204	16.752999	-0.094654	3.541997
495.221796	4257.754401	16.758003	-0.094632	3.538749
495.135978	4249.765966	16.763008	-0.094611	3.535519
495.387456	4241.757422	16.768013	-0.094652	3.532290
495.070617	4233.770549	16.773018	-0.094588	3.529048
495.306440	4225.788568	16.778023	-0.094627	3.525823
495.052158	4217.817846	16.783027	-0.094574	3.522584
495.317875	4209.738094	16.788032	-0.094618	3.519314
495.282513	4201.825155	16.793037	-0.094606	3.516099
495.441393	4193.775360	16.798042	-0.094631	3.512832
495.242868	4185.817677	16.803047	-0.094588	3.509588
495.054612	4177.875072	16.808051	-0.094548	3.506347
494.742241	4169.853960	16.813056	-0.094485	3.503067
494.825577	4161.860591	16.818061	-0.094495	3.499809
494.301899	4153.956936	16.823066	-0.094392	3.496564
494.592207	4145.887286	16.828071	-0.094441	3.493275
494.577472	4137.874475	16.833075	-0.094433	3.489996
494.547135	4129.873494	16.838080	-0.094422	3.486718
494.761016	4121.887993	16.843085	-0.094457	3.483451
494.536056	4113.878031	16.848090	-0.094410	3.480157
494.752298	4105.876890	16.853095	-0.094445	3.476878
494.578505	4097.903894	16.858099	-0.094407	3.473595
494.026698	4089.997767	16.863104	-0.094299	3.470323
494.296724	4081.944403	16.868109	-0.094344	3.467015
494.112082	4073.882396	16.873114	-0.094304	3.463685
494.545637	4065.889271	16.878119	-0.094380	3.460401
494.738918	4057.861116	16.883123	-0.094411	3.457092
494.762474	4049.881561	16.888128	-0.094410	3.453793
495.048813	4041.897968	16.893133	-0.094458	3.450499
494.733425	4033.960574	16.898138	-0.094394	3.447200
493.995277	4026.044541	16.903143	-0.094251	3.443893
494.649230	4017.956574	16.908147	-0.094368	3.440558
494.383934	4010.048812	16.913152	-0.094313	3.437264
494.572813	4001.976165	16.918157	-0.094343	3.433913
494.451849	3994.014188	16.923162	-0.094315	3.430595
494.171915	3986.052202	16.928167	-0.094258	3.427268
493.913137	3978.048438	16.933171	-0.094204	3.423921
493.933520	3970.062235	16.938176	-0.094203	3.420587
494.375027	3962.042636	16.943181	-0.094280	3.417251
493.796608	3954.060169	16.948186	-0.094167	3.413892
493.936361	3946.070986	16.953191	-0.094188	3.410552
494.224186	3938.022010	16.958195	-0.094236	3.407189
493.577986	3930.108742	16.963200	-0.094110	3.403846
493.694634	3922.148709	16.968205	-0.094127	3.400507
493.858482	3914.116726	16.973210	-0.094152	3.397137
493.472286	3906.154939	16.978215	-0.094075	3.393773
493.713596	3898.042607	16.983219	-0.094115	3.390364
493.908293	3890.014090	16.988224	-0.094146	3.386986
493.804729	3882.081112	16.993229	-0.094121	3.383635
493.813470	3874.097672	16.998234	-0.094117	3.380262
493.692707	3866.138490	17.003239	-0.094090	3.376892
493.206386	3858.220268	17.008243	-0.093994	3.373522
492.981696	3850.222809	17.013248	-0.093947	3.370125
493.042727	3842.224995	17.018253	-0.093953	3.366735
493.055354	3834.164447	17.023258	-0.093950	3.363313
492.959638	3826.234577	17.028263	-0.093927	3.359939
492.806899	3818.264146	17.033267	-0.093893	3.356543
492.500749	3810.277151	17.038272	-0.093831	3.353130
492.782273	3802.247035	17.043277	-0.093878	3.349717
492.628684	3794.235331	17.048282	-0.093844	3.346292
492.488789	3786.248235	17.053287	-0.093813	3.342874
493.437008	3778.128329	17.058291	-0.093984	3.339438
492.795147	3770.277650	17.063296	-0.093860	3.336053
492.711140	3762.310909	17.068301	-0.093839	3.332636
492.393001	3754.290935	17.073306	-0.093774	3.329183
492.882138	3746.270952	17.078311	-0.093860	3.325758
493.416880	3738.185253	17.083315	-0.093954	3.322303
493.184956	3730.263854	17.088320	-0.093906	3.318886
493.236859	3722.328977	17.093325	-0.093910	3.315470
492.614822	3714.398229	17.098330	-0.093789	3.312026
492.774076	3706.331419	17.103335	-0.093814	3.308551
492.272108	3698.407619	17.108339	-0.093715	3.305108
492.466163	3690.368235	17.113344	-0.093746	3.301638
492.510670	3682.360818	17.118349	-0.093749	3.298172
492.106237	3674.414696	17.123354	-0.093668	3.294712
492.122746	3666.442511	17.128359	-0.093666	3.291254
492.454008	3658.348784	17.133363	-0.093723	3.287751
492.690905	3650.314465	17.138368	-0.093761	3.284267
492.778088	3642.404747	17.143373	-0.093772	3.280827
492.149402	3634.532289	17.148378	-0.093650	3.277372
491.690966	3626.566270	17.153383	-0.093560	3.273879
491.865336	3618.507223	17.158387	-0.093587	3.270366
492.146602	3610.431202	17.163392	-0.093634	3.266847
491.954411	3602.505140	17.168397	-0.093593	3.263371
491.863984	3594.486325	17.173402	-0.093571	3.259854
492.094176	3586.496295	17.178407	-0.093608	3.256360
492.170392	3578.486394	17.183411	-0.093617	3.252846
491.914994	3570.505332	17.188416	-0.093564	3.249328
492.174703	3562.540311	17.193421	-0.093608	3.245834
491.803798	3554.581054	17.198426	-0.093533	3.242313
491.846974	3546.594674	17.203431	-0.093536	3.238793
492.047448	3538.592299	17.208435	-0.093568	3.235269
492.016834	3530.595569	17.213440	-0.093557	3.231734
492.242510	3522.578516	17.218445	-0.093594	3.228197
491.861874	3514.585128	17.223450	-0.093518	3.224641
492.000552	3506.618464	17.228455	-0.093538	3.221115
491.787321	3498.655866	17.233459	-0.093493	3.217572
491.802880	3490.580693	17.238464	-0.093491	3.213984
491.743975	3482.657701	17.243469	-0.093475	3.210457
491.709946	3474.648586	17.248474	-0.093463	3.206889
491.626320	3466.677643	17.253479	-0.093442	3.203332
490.956743	3458.811578	17.258483	-0.093313	3.199792
491.231802	3450.742368	17.263488	-0.093358	3.196199
491.052602	3442.787175	17.268493	-0.093320	3.192632
490.883425	3434.722942	17.273498	-0.093283	3.189014
491.169962	3426.727640	17.278503	-0.093331	3.185441
491.492881	3418.697327	17.283507	-0.093386	3.181851
490.280692	3410.888645	17.288512	-0.093155	3.178290
490.762356	3402.788119	17.293517	-0.093240	3.174666
490.494810	3394.864451	17.298522	-0.093185	3.171086
490.409750	3386.839338	17.303527	-0.093163	3.167464
490.259249	3378.873392	17.308531	-0.093130	3.163862
490.303633	3370.871277	17.313536	-0.093133	3.160247
490.156648	3362.933625	17.318541	-0.093101	3.156649
490.725055	3354.795616	17.323546	-0.093201	3.152989
490.404300	3346.864457	17.328551	-0.093136	3.149378
490.761316	3338.837859	17.333555	-0.093197	3.145750
490.233850	3330.908503	17.338560	-0.093094	3.142122
490.272012	3322.917440	17.343565	-0.093096	3.138487
490.393490	3314.880088	17.348570	-0.093113	3.134831
490.295658	3306.940911	17.353575	-0.093090	3.131205
489.784174	3299.041278	17.358579	-0.092989	3.127575
490.007280	3290.965107	17.363584	-0.093025	3.123893
490.156817	3283.010008	17.368589	-0.093048	3.120258
489.755584	3275.047825	17.373594	-0.092968	3.116591
489.602688	3267.077757	17.378599	-0.092934	3.112928
490.076756	3258.976617	17.383603	-0.093017	3.109228
489.943301	3251.005843	17.388608	-0.092987	3.105557
489.946552	3243.063962	17.393613	-0.092983	3.101900
489.627089	3235.093039	17.398618	-0.092918	3.098211
490.139287	3227.026477	17.403623	-0.093008	3.094512
489.997640	3219.075577	17.408627	-0.092976	3.090831
490.293453	3211.035058	17.413632	-0.093026	3.087126
490.218065	3203.120721	17.418637	-0.093007	3.083456
489.739434	3195.205915	17.423642	-0.092913	3.079763
489.585963	3187.235303	17.428647	-0.092879	3.076055
490.146790	3179.107146	17.433651	-0.092978	3.072303
490.100927	3171.095896	17.438656	-0.092964	3.068573
489.792287	3163.176374	17.443661	-0.092901	3.064868
489.325392	3155.276895	17.448666	-0.092809	3.061160
489.853051	3147.208967	17.453671	-0.092902	3.057416
489.300145	3139.302560	17.458675	-0.092794	3.053692
489.749462	3131.192181	17.463680	-0.092872	3.049916
489.798052	3123.245729	17.468685	-0.092876	3.046192
489.544672	3115.271950	17.473690	-0.092824	3.042437
489.957283	3107.244651	17.478695	-0.092895	3.038684
489.673726	3099.344235	17.483699	-0.092837	3.034952
489.413217	3091.371144	17.488704	-0.092784	3.031183
489.196658	3083.431276	17.493709	-0.092738	3.027427
489.164036	3075.394193	17.498714	-0.092727	3.023629
489.272151	3067.417063	17.503719	-0.092742	3.019861
489.256518	3059.436529	17.508723	-0.092733	3.016082
489.175298	3051.451882	17.513728	-0.092713	3.012292
489.292450	3043.437925	17.518733	-0.092730	3.008493
489.094785	3035.473981	17.523738	-0.092688	3.004698
489.007638	3027.535997	17.528743	-0.092666	3.000915
488.990089	3019.533875	17.533747	-0.092658	2.997101
488.418255	3011.631137	17.538752	-0.092546	2.993302
488.555024	3003.566381	17.543757	-0.092566	2.989456
488.657738	2995.530579	17.548762	-0.092580	2.985617
488.713149	2987.566801	17.553767	-0.092585	2.981805
488.144183	2979.697809	17.558771	-0.092474	2.978002
488.751060	2971.526825	17.563776	-0.092582	2.974109
488.640163	2963.607755	17.568781	-0.092556	2.970296
488.389566	2955.662159	17.573786	-0.092504	2.966457
488.720168	2947.607151	17.578791	-0.092560	2.962591
488.762989	2939.632454	17.583795	-0.092563	2.958744
488.614834	2931.699816	17.588800	-0.092530	2.954902
488.650136	2923.717651	17.593805	-0.092531	2.951041
488.539020	2915.711652	17.598810	-0.092505	2.947155
488.666458	2907.723024	17.603815	-0.092524	2.943285
488.438622	2899.801020	17.608819	-0.092476	2.939424
488.729725	2891.758958	17.613824	-0.092525	2.935527
488.565295	2883.820316	17.618829	-0.092489	2.931651
488.637398	2875.802943	17.623834	-0.092498	2.927744
488.415644	2867.865001	17.628839	-0.092451	2.923854
488.485280	2859.908786	17.633843	-0.092459	2.919966
488.374438	2851.944217	17.638848	-0.092433	2.916059
488.589574	2843.869689	17.643853	-0.092468	2.912111
488.031600	2835.929211	17.648858	-0.092359	2.908181
488.227947	2827.908358	17.653863	-0.092390	2.904247
487.762343	2820.044155	17.658867	-0.092298	2.900349
487.742536	2812.028460	17.663872	-0.092289	2.896395
487.706970	2804.039380	17.668877	-0.092277	2.892449
487.303629	2796.065769	17.673882	-0.092197	2.888484
487.443458	2788.039939	17.678887	-0.092218	2.884518
487.852054	2780.021960	17.683891	-0.092288	2.880565
487.154491	2772.172447	17.688896	-0.092153	2.876629
486.853683	2764.231010	17.693901	-0.092092	2.872663
487.243598	2756.131281	17.698906	-0.092159	2.868652
486.910021	2748.195772	17.703911	-0.092092	2.864677
486.527722	2740.273227	17.708915	-0.092016	2.860700
486.620719	2732.229381	17.713920	-0.092028	2.856684
487.170084	2724.157414	17.718925	-0.092125	2.852673
487.197627	2716.161478	17.723930	-0.092125	2.848666
486.323082	2708.338018	17.728935	-0.091957	2.844688
486.573773	2700.329860	17.733939	-0.091998	2.840676
486.923995	2692.268207	17.738944	-0.092058	2.836637
487.220322	2684.275374	17.743949	-0.092108	2.832624
486.670547	2676.357440	17.748954	-0.092000	2.828594
486.649211	2668.374303	17.753959	-0.091991	2.824556
486.324528	2660.457856	17.758963	-0.091925	2.820528
485.803335	2652.517731	17.763968	-0.091823	2.816471
485.976376	2644.493768	17.768973	-0.091850	2.812406
486.023274	2636.462169	17.773978	-0.091853	2.808324
486.063713	2628.464408	17.778983	-0.091856	2.804253
486.066713	2620.519284	17.783987	-0.091851	2.800201
485.952486	2612.533943	17.788992	-0.091825	2.796115
485.919221	2604.575908	17.793997	-0.091813	2.792042
486.052743	2596.540618	17.799002	-0.091833	2.787934
486.282574	2588.519217	17.804007	-0.091870	2.783832
486.066351	2580.632773	17.809011	-0.091825	2.779767
485.680855	2572.710539	17.814016	-0.091748	2.775667
485.491947	2564.759576	17.819021	-0.091707	2.771558
485.261024	2556.776491	17.824026	-0.091659	2.767424
485.410198	2548.745577	17.829031	-0.091682	2.763282
485.494816	2540.760153	17.834035	-0.091692	2.759153
485.582534	2532.772425	17.839040	-0.091703	2.755018
485.553984	2524.784575	17.844045	-0.091693	2.750869
485.140629	2516.813047	17.849050	-0.091610	2.746698
485.277519	2508.818426	17.854055	-0.091631	2.742543
485.383010	2500.857522	17.859059	-0.091645	2.738397
485.210555	2492.876651	17.864064	-0.091608	2.734217
485.421014	2484.865936	17.869069	-0.091642	2.730040
485.539490	2476.877767	17.874074	-0.091658	2.725861
485.189255	2468.971003	17.879079	-0.091588	2.721690
484.845267	2461.075807	17.884083	-0.091519	2.717519
485.684069	2452.929888	17.889088	-0.091670	2.713284
485.292172	2445.054991	17.894093	-0.091592	2.709107
485.191548	2437.060453	17.899098	-0.091568	2.704879
484.931663	2429.148430	17.904103	-0.091514	2.700678
484.858463	2421.208028	17.909107	-0.091495	2.696468
484.456831	2413.255174	17.914112	-0.091415	2.692223
484.975556	2405.179936	17.919117	-0.091506	2.687965
484.911495	2397.217909	17.924122	-0.091489	2.683724
484.775490	2389.271994	17.929127	-0.091459	2.679479
484.777473	2381.303225	17.934131	-0.091454	2.675225
484.841491	2373.275382	17.939136	-0.091460	2.670936
484.756614	2365.332770	17.944141	-0.091439	2.666677
484.904756	2357.312131	17.949146	-0.091462	2.662384
484.704909	2349.387672	17.954151	-0.091419	2.658112
484.748577	2341.425274	17.959155	-0.091422	2.653830
484.562799	2333.433340	17.964160	-0.091382	2.649509
484.616834	2325.473227	17.969165	-0.091387	2.645215
485.245849	2317.399358	17.974170	-0.091499	2.640890
485.017215	2309.511191	17.979175	-0.091451	2.636602
484.785885	2301.584579	17.984179	-0.091403	2.632285
484.554306	2293.624355	17.989184	-0.091355	2.627944
484.393735	2285.676334	17.994189	-0.091319	2.623606
484.429684	2277.673906	17.999194	-0.091321	2.619245
484.227038	2269.740786	18.004199	-0.091278	2.614898
484.367583	2261.734807	18.009203	-0.091299	2.610527
484.493972	2253.716597	18.014208	-0.091317	2.606141
484.599834	2245.754435	18.019213	-0.091332	2.601778
484.457469	2237.829315	18.024218	-0.091300	2.597410
484.547527	2229.801769	18.029223	-0.091311	2.592995
483.865940	2221.878675	18.034227	-0.091179	2.588576
483.932215	2213.834671	18.039232	-0.091186	2.584134
483.807939	2205.951035	18.044237	-0.091158	2.579761
484.041835	2197.905933	18.049242	-0.091196	2.575315
483.919719	2189.973813	18.054247	-0.091168	2.570900
484.040568	2181.981435	18.059251	-0.091186	2.566461
484.247480	2173.980972	18.064256	-0.091219	2.562015
484.032897	2166.090300	18.069261	-0.091174	2.557594
483.737068	2158.148466	18.074266	-0.091113	2.553130
483.654838	2150.182884	18.079271	-0.091093	2.548660
483.945169	2142.136789	18.084275	-0.091142	2.544164
483.843384	2134.204252	18.089280	-0.091117	2.539696
484.144868	2126.219957	18.094285	-0.091168	2.535219
483.935917	2118.276918	18.099290	-0.091124	2.530721
484.324911	2110.230749	18.104295	-0.091191	2.526201
484.567914	2102.308119	18.109299	-0.091231	2.521731
483.690621	2094.476399	18.114304	-0.091063	2.517223
483.168278	2086.595325	18.119309	-0.090960	2.512705
483.042618	2078.567919	18.124314	-0.090932	2.508125
483.292611	2070.534781	18.129319	-0.090973	2.503561
483.179999	2062.596975	18.134323	-0.090947	2.499016
483.354755	2054.562276	18.139328	-0.090974	2.494428
483.882934	2046.525379	18.144333	-0.091067	2.489857
483.923073	2038.568355	18.149338	-0.091069	2.485288
483.330770	2030.720329	18.154343	-0.090954	2.480725
482.788869	2022.872951	18.159347	-0.090848	2.476158
482.973176	2014.804254	18.164352	-0.090877	2.471509
483.139935	2006.808671	18.169357	-0.090903	2.466892
483.433194	1998.794411	18.174362	-0.090952	2.462266
483.429858	1990.848207	18.179367	-0.090946	2.457648
483.328522	1982.922328	18.184371	-0.090922	2.453026
482.999519	1974.982358	18.189376	-0.090856	2.448369
483.026098	1967.037460	18.194381	-0.090855	2.443727
483.211176	1959.032622	18.199386	-0.090885	2.439054
482.690799	1951.173571	18.204391	-0.090783	2.434403
482.507318	1943.184133	18.209395	-0.090743	2.429692
482.956756	1935.099287	18.214400	-0.090821	2.424966
483.099232	1927.125410	18.219405	-0.090843	2.420272
482.997887	1919.187226	18.224410	-0.090819	2.415570
483.016449	1911.242250	18.229415	-0.090817	2.410865
482.893271	1903.329059	18.234419	-0.090789	2.406158
482.309168	1895.443483	18.239424	-0.090675	2.401422
482.614938	1887.447369	18.244429	-0.090727	2.396681
482.288568	1879.533862	18.249434	-0.090661	2.391930
482.317969	1871.530909	18.254439	-0.090661	2.387145
482.822004	1863.475995	18.259443	-0.090749	2.382356
482.272754	1855.617703	18.264448	-0.090642	2.377592
482.392896	1847.647682	18.269453	-0.090659	2.372804
482.167743	1839.707966	18.274458	-0.090612	2.367997
482.150477	1831.759751	18.279463	-0.090603	2.363192
482.117913	1823.825912	18.284467	-0.090592	2.358385
481.342136	1815.957142	18.289472	-0.090443	2.353546
481.956935	1807.873124	18.294477	-0.090552	2.348681
481.784318	1799.923530	18.299482	-0.090514	2.343823
481.812897	1791.960822	18.304487	-0.090514	2.338963
481.398208	1784.085793	18.309491	-0.090432	2.334110
481.144538	1776.104962	18.314496	-0.090380	2.329195
481.147935	1768.151402	18.319501	-0.090375	2.324308
481.398930	1760.145947	18.324506	-0.090416	2.319400
481.173229	1752.242857	18.329511	-0.090369	2.314504
481.054875	1744.299017	18.334515	-0.090342	2.309582
480.770626	1736.357002	18.339520	-0.090284	2.304636
481.058636	1728.360174	18.344525	-0.090332	2.299694
480.602103	1720.479264	18.349530	-0.090242	2.294750
480.738602	1712.461474	18.354535	-0.090262	2.289761
480.340260	1704.586917	18.359539	-0.090183	2.284805
480.556076	1696.557521	18.364544	-0.090218	2.279793
480.128066	1688.715885	18.369549	-0.090133	2.274833
479.653185	1680.762588	18.374554	-0.090039	2.269787
480.131902	1672.665974	18.379559	-0.090123	2.264723
480.403184	1664.687806	18.384563	-0.090168	2.259705
480.646294	1656.674963	18.389568	-0.090208	2.254651
480.486746	1648.778633	18.394573	-0.090173	2.249624
480.667014	1640.815764	18.399578	-0.090202	2.244573
480.794050	1632.867129	18.404583	-0.090220	2.239516
480.197697	1625.053410	18.409587	-0.090104	2.234468
480.605868	1617.022238	18.414592	-0.090175	2.229360
480.528800	1609.078865	18.419597	-0.090155	2.224253
480.300566	1601.195899	18.424602	-0.090107	2.219159
480.269975	1593.237316	18.429607	-0.090097	2.214023
480.046859	1585.344410	18.434611	-0.090050	2.208900
479.989219	1577.359464	18.439616	-0.090034	2.203720
480.079934	1569.428479	18.444621	-0.090045	2.198576
479.803667	1561.526576	18.449626	-0.089989	2.193406
479.396202	1553.623410	18.454631	-0.089908	2.188211
479.237526	1545.672701	18.459635	-0.089873	2.182994
479.330122	1537.683448	18.464640	-0.089885	2.177764
479.660567	1529.673468	18.469645	-0.089941	2.172530
479.638749	1521.723353	18.474650	-0.089932	2.167289
479.543083	1513.794288	18.479655	-0.089909	2.162043
479.881949	1505.818558	18.484659	-0.089967	2.156794
479.455031	1497.949181	18.489664	-0.089882	2.151530
479.895760	1489.927507	18.494669	-0.089959	2.146235
479.634594	1482.052097	18.499674	-0.089905	2.140956
479.738984	1474.091451	18.504679	-0.089919	2.135643
479.625362	1466.187746	18.509683	-0.089893	2.130334
479.143954	1458.317899	18.514688	-0.089798	2.124999
479.663120	1450.296291	18.519693	-0.089890	2.119645
479.740183	1442.358730	18.524698	-0.089899	2.114292
479.344247	1434.455147	18.529703	-0.089820	2.108901
479.383359	1426.507338	18.534707	-0.089822	2.103509
479.034069	1418.600078	18.539712	-0.089752	2.098093
479.407999	1410.606242	18.544717	-0.089816	2.092675
479.747655	1402.614094	18.549722	-0.089874	2.087241
479.198819	1394.802266	18.554727	-0.089767	2.081828
478.862606	1386.946332	18.559731	-0.089699	2.076391
478.819147	1378.981588	18.564736	-0.089686	2.070895
479.316764	1370.949094	18.569741	-0.089773	2.065392
479.125765	1363.056532	18.574746	-0.089732	2.059901
479.018911	1355.150360	18.579751	-0.089707	2.054395
478.741841	1347.283079	18.584755	-0.089650	2.048883
478.477258	1339.351001	18.589760	-0.089596	2.043313
478.463894	1331.440645	18.594765	-0.089588	2.037769
478.178803	1323.529778	18.599770	-0.089530	2.032180
478.724703	1315.459914	18.604775	-0.089626	2.026551
478.801264	1307.545866	18.609779	-0.089635	2.020967
478.559444	1299.652580	18.614784	-0.089585	2.015349
478.683805	1291.704561	18.619789	-0.089603	2.009715
478.744108	1283.765026	18.624794	-0.089609	2.004065
478.473012	1275.912358	18.629799	-0.089553	1.998425
478.204114	1268.060617	18.634803	-0.089498	1.992771
477.968412	1260.125751	18.639808	-0.089449	1.987043
478.117564	1252.175942	18.644813	-0.089472	1.981330
478.058034	1244.251851	18.649818	-0.089455	1.975597
478.363477	1236.259174	18.654823	-0.089507	1.969836
477.926782	1228.443904	18.659827	-0.089420	1.964107
477.962501	1220.507127	18.664832	-0.089422	1.958324
478.034492	1212.566756	18.669837	-0.089430	1.952526
477.993158	1204.638453	18.674842	-0.089417	1.946706
477.291814	1196.836450	18.679847	-0.089281	1.940889
477.728055	1188.824304	18.684851	-0.089357	1.935026
478.004868	1180.837796	18.689856	-0.089404	1.929146
478.033459	1172.916679	18.694861	-0.089404	1.923268
477.940396	1165.037298	18.699866	-0.089381	1.917391
477.902848	1157.135313	18.704871	-0.089369	1.911484
477.581051	1149.277385	18.709875	-0.089304	1.905560
477.282333	1141.397286	18.714880	-0.089243	1.899603
477.300630	1133.498233	18.719885	-0.089241	1.893650
476.935120	1125.629276	18.724890	-0.089168	1.887656
476.817158	1117.707985	18.729895	-0.089141	1.881632
477.034842	1109.773764	18.734899	-0.089176	1.875618
476.589105	1101.922131	18.739904	-0.089088	1.869570
476.347210	1094.034942	18.744909	-0.089038	1.863499
476.494382	1086.081951	18.749914	-0.089060	1.857403
476.446548	1078.154517	18.754919	-0.089046	1.851284
476.497213	1070.229094	18.759923	-0.089050	1.845158
476.450205	1062.335301	18.764928	-0.089036	1.839024
476.424569	1054.442944	18.769933	-0.089026	1.832874
476.402365	1046.528276	18.774938	-0.089017	1.826685
475.975518	1038.698929	18.779943	-0.088932	1.820494
476.185564	1030.761235	18.784947	-0.088966	1.814273
476.468034	1022.790370	18.789952	-0.089014	1.808014
476.243156	1014.951417	18.794957	-0.088967	1.801776
476.227486	1007.071240	18.799962	-0.088959	1.795508
476.504660	999.086320	18.804967	-0.089005	1.789172
476.723947	991.173225	18.809971	-0.089041	1.782863
475.722933	983.479744	18.814976	-0.088849	1.776556
475.568580	975.596422	18.819981	-0.088815	1.770179
475.670966	967.669357	18.824986	-0.088829	1.763777
475.405451	959.824044	18.829991	-0.088774	1.757370
475.711646	951.871212	18.834995	-0.088826	1.750926
475.807149	943.949494	18.840000	-0.088839	1.744456
475.050793	936.220872	18.845005	-0.088693	1.738011
475.253198	928.250932	18.850010	-0.088725	1.731466
475.669270	920.282718	18.855015	-0.088798	1.724927
475.199636	912.551857	18.860019	-0.088705	1.718444
474.690034	904.743078	18.865024	-0.088605	1.711866
474.557225	896.842171	18.870029	-0.088575	1.705235
474.851375	888.902537	18.875034	-0.088625	1.698602
475.005764	880.983179	18.880039	-0.088648	1.691942
475.099389	873.089335	18.885043	-0.088660	1.685269
475.264908	865.193575	18.890048	-0.088686	1.678578
475.491519	857.313711	18.895053	-0.088723	1.671881
475.203377	849.495914	18.900058	-0.088664	1.665141
474.984186	841.679112	18.905063	-0.088618	1.658384
475.206962	833.772138	18.910067	-0.088655	1.651582
474.967100	825.947762	18.915072	-0.088605	1.644759
474.810567	818.148441	18.920077	-0.088571	1.637942
475.237379	810.180653	18.925082	-0.088645	1.631030
474.722984	802.393864	18.930087	-0.088544	1.624115
474.553070	794.585293	18.935091	-0.088507	1.617201
474.374904	786.723852	18.940096	-0.088469	1.610208
474.135451	778.917556	18.945101	-0.088419	1.603225
474.218901	771.041569	18.950106	-0.088429	1.596196
473.956618	763.230840	18.955111	-0.088375	1.589144
474.051366	755.360444	18.960115	-0.088388	1.582059
473.660187	747.564753	18.965120	-0.088310	1.574938
473.961021	739.646403	18.970125	-0.088361	1.567775
474.164878	731.770495	18.975130	-0.088393	1.560604
474.021241	723.969163	18.980135	-0.088362	1.553417
474.167218	716.103017	18.985139	-0.088384	1.546180
474.488079	708.211445	18.990144	-0.088438	1.538911
474.066647	700.481610	18.995149	-0.088355	1.531647
474.113217	692.633112	19.000154	-0.088358	1.524307
474.137512	684.816793	19.005159	-0.088358	1.516960
474.218384	677.003617	19.010163	-0.088367	1.509588
473.894581	669.224697	19.015168	-0.088302	1.502149
473.835031	661.426032	19.020173	-0.088286	1.494696
473.481906	653.671304	19.025178	-0.088215	1.487202
473.809251	645.783530	19.030183	-0.088271	1.479649
473.327352	638.069019	19.035187	-0.088176	1.472096
473.684127	630.141027	19.040192	-0.088237	1.464431
473.673134	622.346624	19.045197	-0.088230	1.456797
473.170188	614.642546	19.050202	-0.088131	1.449131
473.044674	606.842776	19.055207	-0.088103	1.441392
472.739694	599.120363	19.060211	-0.088041	1.433659
472.801199	591.271624	19.065216	-0.088047	1.425817
473.023818	583.439358	19.070221	-0.088084	1.417976
473.215590	575.617874	19.075226	-0.088114	1.410097
472.712934	567.935628	19.080231	-0.088015	1.402198
472.346583	560.231961	19.085235	-0.087942	1.394255
472.370469	552.412665	19.090240	-0.087941	1.386215
472.560455	544.607469	19.095245	-0.087972	1.378170
472.263006	536.874086	19.100250	-0.087911	1.370069
472.273729	529.102755	19.105255	-0.087908	1.361934
472.001441	521.411220	19.110259	-0.087852	1.353784
471.886545	513.631840	19.115264	-0.087826	1.345519
472.134349	505.834824	19.120269	-0.087867	1.337250
471.967913	498.110056	19.125274	-0.087831	1.328932
471.867187	490.384087	19.130279	-0.087807	1.320572
471.500168	482.691957	19.135283	-0.087734	1.312147
471.555563	474.867116	19.140288	-0.087739	1.303599
471.750959	467.088154	19.145293	-0.087770	1.295072
471.766818	459.361641	19.150298	-0.087768	1.286513
471.451558	451.701754	19.155303	-0.087704	1.277909
471.530805	443.993682	19.160307	-0.087714	1.269267
471.241752	436.316488	19.165312	-0.087655	1.260530
471.086274	428.649679	19.170317	-0.087621	1.251770
470.532762	421.050984	19.175322	-0.087513	1.242949
470.612195	413.319689	19.180327	-0.087523	1.234035
470.192403	405.689916	19.185331	-0.087439	1.225076
470.168091	397.988416	19.190336	-0.087430	1.216046
470.157912	390.305648	19.195341	-0.087423	1.206973
470.382396	382.584323	19.200346	-0.087460	1.197833
469.765319	375.033000	19.205351	-0.087340	1.188655
470.113609	367.298837	19.210355	-0.087400	1.179383
469.652864	359.723087	19.215360	-0.087309	1.170062
469.827258	352.031184	19.220365	-0.087336	1.160657
469.868976	344.386538	19.225370	-0.087339	1.151206
469.170601	336.858969	19.230375	-0.087204	1.141664
468.763133	329.301092	19.235379	-0.087123	1.132066
467.747361	321.827051	19.240384	-0.086929	1.122360
466.424679	314.419054	19.245389	-0.086678	1.112585
465.173913	306.973486	19.250394	-0.086440	1.102691
463.797306	299.553475	19.255399	-0.086179	1.092711
463.077492	292.013348	19.260403	-0.086040	1.082630
463.152759	284.334390	19.265408	-0.086049	1.072452
462.415728	276.817894	19.270413	-0.085907	1.062205
461.492484	269.360186	19.275418	-0.085730	1.051895
460.489625	261.909392	19.280423	-0.085538	1.041473
459.750251	254.433617	19.285427	-0.085396	1.030973
458.855321	246.970177	19.290432	-0.085224	1.020345
457.977208	239.537223	19.295437	-0.085056	1.009651
456.743200	232.169035	19.300442	-0.084821	0.998847
455.995540	224.680298	19.305447	-0.084677	0.987872
454.899545	217.297191	19.310451	-0.084468	0.976839
452.968484	210.069568	19.315456	-0.084104	0.965693
450.952464	202.863469	19.320461	-0.083724	0.954427
448.815041	195.665036	19.325466	-0.083321	0.943004
446.601543	188.472784	19.330471	-0.082904	0.931429
443.535164	181.443453	19.335475	-0.082328	0.919727
439.595825	174.535522	19.340480	-0.081590	0.907823
435.289435	167.668432	19.345485	-0.080784	0.895721
427.384005	161.390490	19.350490	-0.079308	0.883379
414.911444	155.823987	19.355495	-0.076982	0.870704
398.448971	150.784653	19.360499	-0.073913	0.857541
378.005948	146.239688	19.365504	-0.070104	0.843807
360.320465	141.011116	19.370509	-0.066807	0.829493
348.961476	134.580423	19.375514	-0.064688	0.814768
342.961699	127.243287	19.380519	-0.063566	0.799841
337.584981	119.910887	19.385523	-0.062560	0.784836
329.135708	113.196300	19.390528	-0.060982	0.769670
319.994738	106.641455	19.395533	-0.059276	0.754262
311.022728	100.084537	19.400538	-0.057601	0.738580
303.458331	93.332107	19.405543	-0.056188	0.722660
297.818107	86.501970	19.410547	-0.055133	0.706916