Mon Apr 19 09:50:02 2021

Number of Points = 3633
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.886397	0.003433	0.000000	0.000069	0.313320

1.612409	0.052143	0.005005	0.000120	0.313315
1.255473	0.118507	0.010010	0.000186	0.313322
1.541534	0.067608	0.015014	0.000133	0.313327
1.577481	0.055820	0.020019	0.000126	0.313302
1.744097	0.025352	0.025024	0.000095	0.313301
1.189659	0.127317	0.030029	0.000199	0.313307
1.769136	0.020118	0.035034	0.000091	0.313298
1.530854	0.065544	0.040038	0.000135	0.313308
1.714439	0.025985	0.045043	0.000101	0.313279
2.064767	-0.034891	0.050048	0.000036	0.313291
1.808787	0.012790	0.055053	0.000083	0.313297
1.634811	0.046187	0.060058	0.000116	0.313305
1.562524	0.059374	0.065062	0.000129	0.313305
1.516001	0.068899	0.070067	0.000138	0.313310
1.845053	0.009010	0.075072	0.000077	0.313309
1.444416	0.081632	0.080077	0.000151	0.313308
1.852040	0.003764	0.085082	0.000076	0.313290
2.328026	-0.137049	0.090086	-0.000013	0.313039
2.243488	-0.132385	0.095091	0.000003	0.312990
2.061396	-0.094860	0.100096	0.000037	0.313010
1.953391	-0.078984	0.105101	0.000057	0.312993
1.781048	-0.048047	0.110106	0.000089	0.312991
2.151217	-0.113455	0.115110	0.000020	0.312999
1.764775	-0.087842	0.120115	0.000092	0.312793
1.672617	-0.095716	0.125120	0.000109	0.312679
1.579584	-0.081810	0.130125	0.000127	0.312665
1.362177	-0.038835	0.135130	0.000167	0.312681
1.553285	-0.071597	0.140134	0.000132	0.312690
0.959408	0.035044	0.145139	0.000242	0.312684
1.224342	-0.065096	0.150144	0.000193	0.312443
1.044501	-0.049131	0.155149	0.000226	0.312365
0.827991	-0.005976	0.160154	0.000267	0.312383
1.097589	-0.055848	0.165158	0.000217	0.312378
1.527194	-0.141344	0.170163	0.000137	0.312344
1.593321	-0.192538	0.175168	0.000125	0.312162
1.498871	-0.204084	0.180173	0.000142	0.312029
1.677232	-0.236690	0.185178	0.000109	0.312028
2.025561	-0.298962	0.190182	0.000044	0.312032
1.688221	-0.295991	0.195187	0.000107	0.311762
1.750890	-0.311708	0.200192	0.000095	0.311741
1.879181	-0.337130	0.205197	0.000072	0.311731
1.405446	-0.289281	0.210202	0.000160	0.311554
1.136195	-0.273036	0.215206	0.000210	0.311402
1.254746	-0.296511	0.220211	0.000188	0.311393
1.672785	-0.386091	0.225216	0.000110	0.311329
0.976892	-0.311073	0.230221	0.000240	0.311090
1.035340	-0.320455	0.235226	0.000229	0.311096
1.670091	-0.441301	0.240230	0.000111	0.311070
1.665896	-0.507719	0.245235	0.000112	0.310757
1.267390	-0.429966	0.250240	0.000186	0.310782
1.217725	-0.435835	0.255245	0.000195	0.310712
1.324031	-0.493806	0.260250	0.000175	0.310532
1.396974	-0.506769	0.265254	0.000162	0.310533
1.295859	-0.532131	0.270259	0.000181	0.310329
0.554456	-0.422716	0.275264	0.000319	0.310211
1.189076	-0.545563	0.280269	0.000201	0.310176
0.982362	-0.567331	0.285274	0.000239	0.309899
0.672431	-0.517320	0.290278	0.000297	0.309870
-0.145973	-0.378332	0.295283	0.000449	0.309824
0.437146	-0.543963	0.300288	0.000341	0.309545
1.104828	-0.668783	0.305293	0.000217	0.309529
1.107390	-0.706414	0.310298	0.000216	0.309355
0.646814	-0.641970	0.315302	0.000302	0.309264
0.605018	-0.655941	0.320307	0.000310	0.309163
0.974334	-0.777040	0.325312	0.000241	0.308910
0.673874	-0.721245	0.330317	0.000297	0.308916
0.499913	-0.755793	0.335322	0.000330	0.308606
0.533686	-0.762358	0.340326	0.000323	0.308604
0.287831	-0.768843	0.345331	0.000369	0.308364
0.313707	-0.788831	0.350336	0.000364	0.308292
0.406908	-0.839449	0.355341	0.000347	0.308133
0.225824	-0.837176	0.360346	0.000381	0.307989
-0.132927	-0.789221	0.365350	0.000448	0.307908
0.339791	-0.930056	0.370355	0.000360	0.307650
0.154828	-0.906634	0.375360	0.000394	0.307602
0.340814	-0.997662	0.380365	0.000360	0.307332
0.109915	-0.967633	0.385370	0.000403	0.307276
-0.110984	-0.980284	0.390374	0.000444	0.307027
-0.116756	-0.992883	0.395379	0.000445	0.306963
-0.398787	-0.992978	0.400384	0.000498	0.306721
-0.265056	-1.025256	0.405389	0.000473	0.306683
-0.241740	-1.092453	0.410394	0.000468	0.306385
0.060749	-1.158803	0.415398	0.000412	0.306332
-0.273687	-1.152639	0.420403	0.000474	0.306073
-0.357796	-1.152797	0.425408	0.000490	0.306000
-0.758536	-1.127526	0.430413	0.000565	0.305775
-0.737378	-1.148647	0.435418	0.000561	0.305693
-0.521077	-1.223991	0.440422	0.000521	0.305523
-1.131411	-1.145702	0.445427	0.000634	0.305368
-0.993014	-1.208666	0.450432	0.000609	0.305189
-1.069561	-1.232432	0.455437	0.000623	0.305010
-1.586993	-1.168353	0.460442	0.000719	0.304867
-1.759604	-1.178460	0.465446	0.000751	0.304670
-2.209443	-1.125934	0.470451	0.000835	0.304532
-1.960734	-1.202961	0.475456	0.000789	0.304380
-2.226068	-1.179285	0.480461	0.000838	0.304263
-2.259431	-1.214990	0.485466	0.000845	0.304064
-1.957912	-1.300044	0.490470	0.000789	0.303920
-2.213056	-1.294684	0.495475	0.000836	0.303725
-1.629913	-1.425931	0.500480	0.000728	0.303604
-2.091578	-1.396492	0.505485	0.000814	0.303344
-1.841170	-1.455605	0.510490	0.000767	0.303279
-2.059287	-1.475453	0.515494	0.000808	0.302995
-2.345664	-1.440788	0.520499	0.000861	0.302912
-2.719528	-1.425517	0.525504	0.000931	0.302660
-3.066147	-1.387695	0.530509	0.000995	0.302540
-3.622564	-1.326692	0.535514	0.001099	0.302348
-3.371920	-1.399026	0.540518	0.001052	0.302219
-3.582970	-1.401808	0.545523	0.001092	0.302022
-3.629822	-1.419701	0.550528	0.001100	0.301896
-3.912306	-1.400655	0.555533	0.001153	0.301741
-3.580817	-1.496523	0.560538	0.001091	0.301570
-3.069960	-1.622704	0.565542	0.000996	0.301409
-3.562718	-1.581353	0.570547	0.001088	0.301178
-3.644132	-1.582590	0.575552	0.001103	0.301101
-3.884306	-1.602702	0.580557	0.001148	0.300794
-3.648478	-1.657958	0.585562	0.001104	0.300734
-3.482707	-1.729276	0.590566	0.001074	0.300536
-4.343576	-1.608199	0.595571	0.001234	0.300365
-5.014757	-1.522246	0.600576	0.001359	0.300191
-4.495606	-1.652705	0.605581	0.001262	0.300017
-3.767300	-1.817095	0.610586	0.001127	0.299863
-3.918986	-1.843756	0.615590	0.001155	0.299601
-4.749977	-1.712826	0.620595	0.001310	0.299503
-4.927582	-1.729686	0.625600	0.001343	0.299266
-5.023717	-1.733325	0.630605	0.001361	0.299163
-4.998441	-1.786106	0.635610	0.001356	0.298930
-5.276549	-1.769285	0.640614	0.001408	0.298767
-5.820291	-1.701285	0.645619	0.001509	0.298617
-5.736911	-1.762095	0.650624	0.001494	0.298396
-5.414022	-1.839199	0.655629	0.001434	0.298306
-5.745688	-1.834955	0.660634	0.001495	0.298034
-6.153423	-1.771978	0.665638	0.001571	0.297980
-6.376545	-1.796929	0.670643	0.001613	0.297662
-5.573971	-1.963955	0.675648	0.001464	0.297559
-5.791393	-1.970662	0.680653	0.001504	0.297334
-5.786670	-2.013758	0.685658	0.001503	0.297128
-6.039943	-1.989462	0.690662	0.001551	0.297022
-6.816954	-1.906661	0.695667	0.001695	0.296737
-6.618279	-1.955160	0.700672	0.001658	0.296676
-6.801402	-1.978607	0.705677	0.001692	0.296399
-6.519520	-2.059161	0.710682	0.001640	0.296256
-7.199773	-1.969245	0.715686	0.001767	0.296091
-7.624879	-1.935882	0.720691	0.001846	0.295876
-7.856100	-1.914861	0.725696	0.001889	0.295773
-8.053976	-1.916692	0.730701	0.001926	0.295588
-8.431713	-1.858042	0.735706	0.001996	0.295539
-8.193597	-1.958815	0.740710	0.001952	0.295257
-9.112660	-1.805428	0.745715	0.002123	0.295190
-8.448000	-1.981911	0.750720	0.001999	0.294917
-8.366595	-2.008162	0.755725	0.001984	0.294861
-9.418710	-1.879845	0.760730	0.002180	0.294551
-9.741929	-1.816984	0.765734	0.002240	0.294571
-9.957505	-1.833019	0.770739	0.002280	0.294300
-9.829984	-1.861192	0.775744	0.002257	0.294275
-10.194001	-1.850357	0.780749	0.002325	0.294003
-10.434366	-1.820103	0.785754	0.002369	0.293936
-10.075125	-1.925451	0.790758	0.002303	0.293739
-10.727864	-1.831687	0.795763	0.002424	0.293616
-10.782938	-1.850774	0.800768	0.002434	0.293473
-10.889486	-1.865814	0.805773	0.002454	0.293303
-10.899661	-1.887165	0.810778	0.002456	0.293188
-10.956572	-1.914663	0.815782	0.002467	0.293001
-11.079071	-1.908531	0.820787	0.002490	0.292921
-11.284163	-1.923851	0.825792	0.002528	0.292661
-11.259902	-1.937453	0.830797	0.002523	0.292616
-11.319957	-1.983377	0.835802	0.002535	0.292334
-11.200888	-2.007147	0.840806	0.002513	0.292323
-11.787731	-1.963960	0.845811	0.002622	0.292009
-11.713138	-1.976777	0.850816	0.002608	0.292012
-12.030575	-1.975522	0.855821	0.002667	0.291732
-12.057440	-1.972179	0.860826	0.002672	0.291724
-12.668844	-1.915694	0.865830	0.002786	0.291453
-12.308795	-1.993860	0.870835	0.002719	0.291390
-12.140200	-2.069340	0.875840	0.002688	0.291167
-12.773311	-1.971456	0.880845	0.002806	0.291081
-12.874218	-1.992635	0.885850	0.002824	0.290884
-12.852379	-2.019549	0.890854	0.002820	0.290770
-13.030796	-2.014038	0.895859	0.002854	0.290636
-13.178616	-2.013218	0.900864	0.002881	0.290506
-13.095159	-2.051147	0.905869	0.002866	0.290392
-14.100487	-1.910769	0.910874	0.003053	0.290181
-14.098617	-1.913567	0.915878	0.003053	0.290169
-14.376884	-1.924339	0.920883	0.003104	0.289862
-14.665873	-1.867652	0.925888	0.003158	0.289883
-15.120421	-1.828398	0.930893	0.003243	0.289666
-15.047978	-1.867065	0.935898	0.003229	0.289538
-14.386726	-2.001582	0.940902	0.003106	0.289467
-14.556398	-2.016906	0.945907	0.003138	0.289236
-14.820796	-1.968855	0.950912	0.003187	0.289235
-15.147148	-1.974436	0.955917	0.003248	0.288910
-15.275802	-1.951701	0.960922	0.003272	0.288907
-15.671388	-1.918863	0.965926	0.003346	0.288711
-16.211123	-1.842768	0.970931	0.003446	0.288600
-15.564854	-1.974363	0.975936	0.003326	0.288529
-15.815447	-1.980211	0.980941	0.003373	0.288271
-15.840247	-1.977317	0.985946	0.003377	0.288263
-16.070756	-1.983782	0.990950	0.003420	0.288020
-16.415271	-1.929384	0.995955	0.003484	0.287978
-16.462747	-1.954247	1.000960	0.003493	0.287810
-16.323107	-2.014991	1.005965	0.003467	0.287632
-16.841186	-1.928567	1.010970	0.003564	0.287592
-17.201349	-1.915008	1.015974	0.003631	0.287331
-17.473418	-1.864544	1.020979	0.003682	0.287336
-16.946396	-2.002074	1.025984	0.003584	0.287125
-17.459244	-1.932007	1.030989	0.003679	0.287008
-17.439357	-1.947660	1.035994	0.003675	0.286947
-17.370014	-2.002805	1.040998	0.003663	0.286733
-17.990218	-1.891112	1.046003	0.003778	0.286727
-18.115827	-1.916915	1.051008	0.003801	0.286481
-18.384410	-1.885577	1.056013	0.003852	0.286393
-18.608175	-1.848580	1.061018	0.003893	0.286374
-18.251823	-1.972582	1.066022	0.003827	0.286074
-18.300503	-1.967813	1.071027	0.003836	0.286054
-18.026551	-2.058460	1.076032	0.003785	0.285847
-18.505372	-1.992654	1.081037	0.003874	0.285739
-18.540557	-2.001853	1.086042	0.003881	0.285660
-18.622816	-2.017695	1.091046	0.003896	0.285503
-18.834683	-1.980021	1.096051	0.003936	0.285499
-19.567724	-1.905502	1.101056	0.004072	0.285201
-19.405572	-1.943941	1.106061	0.004042	0.285155
-18.918812	-2.064160	1.111066	0.003952	0.284994
-19.607036	-1.968673	1.116070	0.004080	0.284843
-19.623849	-1.968443	1.121075	0.004083	0.284829
-19.568612	-2.038803	1.126080	0.004073	0.284522
-19.531756	-2.048654	1.131085	0.004066	0.284506
-19.841014	-2.028178	1.136090	0.004123	0.284324
-20.036587	-2.012361	1.141094	0.004160	0.284223
-19.888158	-2.057867	1.146099	0.004132	0.284128
-20.478946	-1.997336	1.151104	0.004242	0.283889
-20.762900	-1.943916	1.156109	0.004295	0.283898
-20.880647	-1.966744	1.161114	0.004317	0.283672
-20.852947	-1.989644	1.166118	0.004312	0.283581
-21.194617	-1.939668	1.171123	0.004376	0.283519
-21.093129	-2.009483	1.176128	0.004357	0.283256
-20.840810	-2.056978	1.181133	0.004310	0.283248
-21.475581	-1.984391	1.186138	0.004428	0.283029
-21.297954	-2.029964	1.191142	0.004395	0.282961
-21.331929	-2.044179	1.196147	0.004401	0.282856
-21.457867	-2.067624	1.201152	0.004425	0.282619
-21.591218	-2.044652	1.206157	0.004450	0.282612
-22.145961	-1.997810	1.211162	0.004553	0.282335
-22.009509	-2.027298	1.216166	0.004528	0.282311
-22.273177	-2.006120	1.221171	0.004577	0.282174
-22.410077	-2.017158	1.226176	0.004602	0.281989
-22.551177	-1.990192	1.231181	0.004629	0.281996
-23.029556	-1.953689	1.236186	0.004718	0.281736
-22.817807	-2.000693	1.241190	0.004678	0.281692
-22.668296	-2.048482	1.246195	0.004651	0.281586
-23.232291	-1.989154	1.251200	0.004756	0.281364
-23.233772	-1.988995	1.256205	0.004756	0.281363
-23.621748	-1.963172	1.261210	0.004828	0.281133
-23.698827	-1.960168	1.266214	0.004843	0.281076
-23.736496	-1.963200	1.271219	0.004850	0.281025
-23.971878	-1.973598	1.276224	0.004893	0.280750
-24.399986	-1.892683	1.281229	0.004973	0.280766
-24.820959	-1.831335	1.286234	0.005052	0.280688
-24.928555	-1.838820	1.291238	0.005072	0.280548
-24.607375	-1.900942	1.296243	0.005012	0.280528
-24.714497	-1.916782	1.301248	0.005032	0.280346
-25.284378	-1.843254	1.306253	0.005138	0.280190
-24.867070	-1.920350	1.311258	0.005060	0.280184
-24.732951	-1.992401	1.316262	0.005035	0.279937
-25.356828	-1.895839	1.321267	0.005152	0.279850
-24.897894	-1.988873	1.326272	0.005066	0.279800
-25.257556	-1.972545	1.331277	0.005133	0.279546
-26.014712	-1.834647	1.336282	0.005274	0.279547
-25.804327	-1.896210	1.341286	0.005235	0.279426
-26.494701	-1.801769	1.346291	0.005364	0.279265
-25.860008	-1.919513	1.351296	0.005246	0.279252
-25.869553	-1.960083	1.356301	0.005247	0.279033
-26.427532	-1.883135	1.361306	0.005351	0.278906
-26.336885	-1.896276	1.366310	0.005334	0.278923
-26.486607	-1.926616	1.371315	0.005362	0.278624
-26.482681	-1.933000	1.376320	0.005362	0.278594
-26.718637	-1.901032	1.381325	0.005406	0.278537
-26.933464	-1.911880	1.386330	0.005446	0.278277
-27.176611	-1.863211	1.391334	0.005491	0.278300
-27.501769	-1.828153	1.396339	0.005551	0.278175
-27.428102	-1.874323	1.401344	0.005538	0.278004
-27.909022	-1.785182	1.406349	0.005627	0.278013
-28.406174	-1.721785	1.411354	0.005720	0.277872
-27.980286	-1.834408	1.416358	0.005641	0.277688
-28.392422	-1.762196	1.421363	0.005717	0.277674
-28.520859	-1.762182	1.426368	0.005741	0.277552
-28.320164	-1.835754	1.431373	0.005704	0.277358
-28.213285	-1.857328	1.436378	0.005684	0.277347
-28.652296	-1.808719	1.441382	0.005766	0.277184
-28.823983	-1.809938	1.446387	0.005798	0.277014
-27.807044	-1.996448	1.451392	0.005609	0.277006
-28.432754	-1.926645	1.456397	0.005725	0.276776
-28.810999	-1.868475	1.461402	0.005796	0.276720
-28.343440	-1.966943	1.466406	0.005709	0.276649
-28.838379	-1.929211	1.471411	0.005801	0.276375
-28.767849	-1.939888	1.476416	0.005788	0.276387
-28.604268	-2.006705	1.481421	0.005757	0.276192
-29.182061	-1.923930	1.486426	0.005865	0.276075
-29.228415	-1.919143	1.491430	0.005874	0.276056
-29.320807	-1.959474	1.496435	0.005891	0.275756
-29.110136	-1.997807	1.501440	0.005852	0.275756
-29.906400	-1.874582	1.506445	0.006000	0.275642
-30.048610	-1.872985	1.511450	0.006026	0.275514
-29.662060	-1.938572	1.516454	0.005955	0.275539
-30.219520	-1.895737	1.521459	0.006058	0.275231
-30.192787	-1.911866	1.526464	0.006053	0.275172
-30.271383	-1.909591	1.531469	0.006068	0.275108
-30.312131	-1.950067	1.536474	0.006076	0.274856
-29.927893	-2.019331	1.541478	0.006004	0.274859
-30.369926	-1.986890	1.546483	0.006087	0.274606
-30.572489	-1.965058	1.551488	0.006124	0.274527
-30.438317	-2.003564	1.556493	0.006099	0.274452
-30.812414	-1.977806	1.561498	0.006169	0.274229
-30.363120	-2.058010	1.566502	0.006086	0.274237
-31.126567	-1.973287	1.571507	0.006228	0.273951
-31.089204	-1.991267	1.576512	0.006221	0.273891
-30.804494	-2.064143	1.581517	0.006168	0.273780
-31.785433	-1.919771	1.586522	0.006350	0.273599
-31.860977	-1.906162	1.591526	0.006365	0.273599
-32.205963	-1.889277	1.596531	0.006429	0.273356
-31.963118	-1.947292	1.601536	0.006384	0.273282
-32.238566	-1.900670	1.606541	0.006435	0.273264
-32.846644	-1.840459	1.611546	0.006548	0.272996
-32.602504	-1.882703	1.616550	0.006503	0.273008
-32.842025	-1.861121	1.621555	0.006547	0.272891
-33.274402	-1.823828	1.626560	0.006628	0.272671
-32.992623	-1.875198	1.631565	0.006575	0.272670
-32.993565	-1.909211	1.636570	0.006576	0.272489
-33.470069	-1.846557	1.641574	0.006664	0.272361
-33.481203	-1.846580	1.646579	0.006667	0.272350
-33.402404	-1.908587	1.651584	0.006652	0.272096
-33.566979	-1.890678	1.656589	0.006683	0.272032
-33.605196	-1.894427	1.661594	0.006690	0.271975
-33.282164	-1.999029	1.666598	0.006630	0.271730
-33.404947	-1.979133	1.671603	0.006653	0.271717
-33.841908	-1.939947	1.676608	0.006734	0.271502
-33.764762	-1.974989	1.681613	0.006720	0.271390
-33.690088	-1.997990	1.686618	0.006706	0.271340
-34.336945	-1.926777	1.691622	0.006826	0.271091
-34.753817	-1.852610	1.696627	0.006904	0.271082
-34.308550	-1.963122	1.701632	0.006821	0.270924
-34.277007	-1.998561	1.706637	0.006815	0.270766
-34.918883	-1.881476	1.711642	0.006935	0.270767
-34.840816	-1.940010	1.716646	0.006920	0.270530
-35.045189	-1.904625	1.721651	0.006958	0.270520
-35.004392	-1.938034	1.726656	0.006951	0.270381
-35.492691	-1.886974	1.731661	0.007042	0.270178
-35.025575	-1.974844	1.736666	0.006955	0.270163
-35.738998	-1.887967	1.741670	0.007088	0.269932
-36.375416	-1.784483	1.746675	0.007206	0.269866
-35.983504	-1.855123	1.751680	0.007133	0.269870
-36.591683	-1.801387	1.756685	0.007246	0.269564
-37.051243	-1.720108	1.761690	0.007332	0.269552
-36.560329	-1.810779	1.766694	0.007241	0.269544
-36.349528	-1.903293	1.771699	0.007202	0.269253
-36.869951	-1.805974	1.776704	0.007298	0.269267
-36.782572	-1.841861	1.781709	0.007282	0.269159
-36.912955	-1.862126	1.786714	0.007307	0.268922
-36.602490	-1.916973	1.791718	0.007249	0.268931
-37.453252	-1.799672	1.796723	0.007407	0.268729
-38.053325	-1.707971	1.801728	0.007519	0.268635
-38.178016	-1.679832	1.806733	0.007542	0.268664
-38.103222	-1.735270	1.811738	0.007528	0.268438
-38.080753	-1.762605	1.816742	0.007524	0.268313
-38.246536	-1.732414	1.821747	0.007555	0.268313
-38.140325	-1.783921	1.826752	0.007535	0.268139
-38.796624	-1.683199	1.831757	0.007657	0.268038
-38.720348	-1.698083	1.836762	0.007643	0.268032
-38.805530	-1.717316	1.841766	0.007659	0.267844
-39.793063	-1.563904	1.846771	0.007843	0.267702
-39.174074	-1.678174	1.851776	0.007728	0.267693
-38.988042	-1.733572	1.856781	0.007693	0.267576
-40.074399	-1.569774	1.861786	0.007895	0.267393
-39.574526	-1.660094	1.866790	0.007803	0.267396
-39.310028	-1.727164	1.871795	0.007753	0.267293
-40.020405	-1.640368	1.876800	0.007886	0.267063
-39.872403	-1.666733	1.881805	0.007858	0.267066
-39.774824	-1.699625	1.886810	0.007840	0.266984
-39.611016	-1.769719	1.891814	0.007810	0.266765
-39.479910	-1.796462	1.896819	0.007785	0.266749
-39.335426	-1.858236	1.901824	0.007758	0.266556
-40.074562	-1.747099	1.906829	0.007896	0.266429
-40.708245	-1.629968	1.911834	0.008014	0.266439
-40.686523	-1.672068	1.916838	0.008010	0.266231
-40.738686	-1.682717	1.921843	0.008020	0.266122
-41.078691	-1.617934	1.926848	0.008083	0.266138
-41.156523	-1.643204	1.931853	0.008098	0.265923
-41.338077	-1.630178	1.936858	0.008131	0.265814
-40.682397	-1.750332	1.941862	0.008009	0.265809
-41.556568	-1.625430	1.946867	0.008172	0.265623
-41.765671	-1.598887	1.951872	0.008211	0.265560
-41.272856	-1.689848	1.956877	0.008119	0.265552
-41.350324	-1.727523	1.961882	0.008134	0.265270
-41.534914	-1.706078	1.966886	0.008168	0.265203
-41.681147	-1.681442	1.971891	0.008195	0.265192
-41.627461	-1.746626	1.976896	0.008186	0.264889
-41.974795	-1.681959	1.981901	0.008250	0.264897
-41.760849	-1.742906	1.986906	0.008210	0.264777
-42.010111	-1.736184	1.991910	0.008257	0.264565
-42.134407	-1.716064	1.996915	0.008280	0.264551
-41.941781	-1.793175	2.001920	0.008244	0.264321

-42.307686	-1.758617	2.011917	0.008312	0.264145
-42.236975	-1.813258	2.021914	0.008299	0.263915
-42.933454	-1.728233	2.031910	0.008429	0.263686
-43.484122	-1.636049	2.041907	0.008532	0.263642
-42.850419	-1.788669	2.051904	0.008414	0.263437
-43.045812	-1.779272	2.061901	0.008450	0.263292
-43.187203	-1.755474	2.071898	0.008477	0.263281
-43.935774	-1.666217	2.081894	0.008616	0.263023
-43.736591	-1.702294	2.091891	0.008579	0.263023
-44.075743	-1.639532	2.101888	0.008642	0.263029
-43.806026	-1.690626	2.111885	0.008592	0.263017
-43.428579	-1.761147	2.121882	0.008522	0.263007
-43.422862	-1.764388	2.131878	0.008521	0.262994
-43.598409	-1.790760	2.141875	0.008554	0.262673
-44.069039	-1.704610	2.151872	0.008641	0.262675
-43.457795	-1.818647	2.161869	0.008528	0.262659
-43.851300	-1.742037	2.171866	0.008601	0.262686
-43.759273	-1.698760	2.181862	0.008584	0.263017
-44.012070	-1.649943	2.191859	0.008631	0.263032
-43.988049	-1.655609	2.201856	0.008627	0.263025
-43.730556	-1.703898	2.211853	0.008579	0.263016
-43.467341	-1.753064	2.221850	0.008530	0.263009
-43.859950	-1.673573	2.231846	0.008603	0.263053
-43.293721	-1.730329	2.241843	0.008498	0.263307
-43.114733	-1.765478	2.251840	0.008464	0.263292
-43.227747	-1.743052	2.261837	0.008485	0.263302
-43.370775	-1.703191	2.271834	0.008512	0.263378
-43.024711	-1.721090	2.281830	0.008448	0.263625
-43.191056	-1.689769	2.291827	0.008479	0.263631
-42.789086	-1.745887	2.301824	0.008404	0.263724
-42.472408	-1.765781	2.311821	0.008345	0.263930
-42.587329	-1.746761	2.321818	0.008367	0.263920
-42.513148	-1.717861	2.331814	0.008353	0.264152
-41.943430	-1.802769	2.341811	0.008247	0.264254
-41.913950	-1.804325	2.351808	0.008242	0.264275
-41.844774	-1.767783	2.361805	0.008229	0.264543
-41.480703	-1.837721	2.371802	0.008161	0.264523
-40.940663	-1.896300	2.381798	0.008061	0.264739
-41.046786	-1.855838	2.391795	0.008080	0.264855
-41.153204	-1.819717	2.401792	0.008100	0.264946
-40.700888	-1.860070	2.411789	0.008016	0.265175
-40.942854	-1.810734	2.421786	0.008061	0.265203
-40.763012	-1.784499	2.431782	0.008028	0.265525
-40.630350	-1.799800	2.441779	0.008003	0.265572
-40.496156	-1.785465	2.451776	0.007978	0.265783
-40.461283	-1.770922	2.461773	0.007972	0.265897
-40.274037	-1.767151	2.471770	0.007937	0.266102
-39.771086	-1.825561	2.481766	0.007843	0.266282
-39.474829	-1.858885	2.491763	0.007788	0.266393
-39.274423	-1.848051	2.501760	0.007751	0.266650
-39.509856	-1.784028	2.511757	0.007795	0.266765
-39.887365	-1.662631	2.521754	0.007865	0.267050
-39.470211	-1.704403	2.531750	0.007788	0.267235
-39.025167	-1.758887	2.541747	0.007705	0.267378
-38.967210	-1.712538	2.551744	0.007694	0.267685
-38.221180	-1.819318	2.561741	0.007555	0.267841
-38.131523	-1.804287	2.571738	0.007539	0.268010
-37.904242	-1.799173	2.581734	0.007496	0.268261
-37.680820	-1.816669	2.591731	0.007455	0.268385
-37.450386	-1.814172	2.601728	0.007412	0.268625
-37.738492	-1.717362	2.611725	0.007466	0.268864
-37.354448	-1.757740	2.621722	0.007394	0.269022
-36.688870	-1.832774	2.631718	0.007271	0.269269
-37.043687	-1.726866	2.641715	0.007337	0.269491
-36.595837	-1.775555	2.651712	0.007253	0.269667
-36.183838	-1.810747	2.661709	0.007177	0.269880
-36.325666	-1.732451	2.671706	0.007203	0.270161
-36.069769	-1.739893	2.681702	0.007156	0.270370
-35.764591	-1.756621	2.691699	0.007099	0.270577
-35.912120	-1.683643	2.701696	0.007126	0.270824
-35.728400	-1.672042	2.711693	0.007092	0.271064
-35.452386	-1.683047	2.721690	0.007041	0.271273
-34.825344	-1.761593	2.731686	0.006924	0.271462
-34.955290	-1.679312	2.741683	0.006948	0.271774
-34.923852	-1.639042	2.751680	0.006943	0.272019
-34.840733	-1.607211	2.761677	0.006927	0.272268
-34.245311	-1.677946	2.771674	0.006816	0.272468
-34.073178	-1.663951	2.781670	0.006784	0.272708
-33.501352	-1.708310	2.791667	0.006678	0.273024
-32.892918	-1.785035	2.801664	0.006565	0.273203
-33.571860	-1.615949	2.811661	0.006691	0.273445
-32.825000	-1.714997	2.821658	0.006552	0.273639
-32.807270	-1.658406	2.831654	0.006549	0.273955
-32.778785	-1.616351	2.841651	0.006544	0.274204
-32.265850	-1.666153	2.851648	0.006448	0.274433
-31.956745	-1.683802	2.861645	0.006391	0.274636
-31.969750	-1.627614	2.871642	0.006393	0.274920
-31.182832	-1.718849	2.881638	0.006247	0.275192
-30.766567	-1.758712	2.891635	0.006170	0.275380
-30.780688	-1.711509	2.901632	0.006172	0.275615
-30.623374	-1.702823	2.911629	0.006143	0.275810
-30.291513	-1.712701	2.921626	0.006081	0.276075
-30.051158	-1.718176	2.931622	0.006037	0.276275
-29.957329	-1.694429	2.941619	0.006019	0.276488
-29.354659	-1.753275	2.951616	0.005907	0.276753
-29.500763	-1.680750	2.961613	0.005934	0.276993
-28.721856	-1.782293	2.971610	0.005789	0.277202
-28.778643	-1.735149	2.981606	0.005800	0.277394
-27.961471	-1.831664	2.991603	0.005648	0.277666
-27.672797	-1.842710	3.001600	0.005594	0.277881
-27.685094	-1.806135	3.011597	0.005597	0.278060
-27.918148	-1.714362	3.021594	0.005640	0.278317
-27.366240	-1.763988	3.031590	0.005537	0.278580
-26.977155	-1.801754	3.041587	0.005465	0.278751
-26.583900	-1.836685	3.051584	0.005392	0.278941
-26.591250	-1.772502	3.061581	0.005393	0.279266
-26.388205	-1.770078	3.071578	0.005356	0.279470
-26.791524	-1.655811	3.081574	0.005431	0.279681
-26.095202	-1.738504	3.091571	0.005301	0.279908
-25.746880	-1.743930	3.101568	0.005236	0.280207
-25.474858	-1.748005	3.111565	0.005186	0.280441
-25.703949	-1.665311	3.121562	0.005228	0.280653
-25.347742	-1.695564	3.131558	0.005162	0.280830
-24.674494	-1.766293	3.141555	0.005037	0.281096
-24.433159	-1.764107	3.151552	0.004992	0.281333
-23.982114	-1.806651	3.161549	0.004908	0.281536
-23.470775	-1.864308	3.171546	0.004813	0.281717
-23.667432	-1.771817	3.181542	0.004850	0.282008
-23.574418	-1.747152	3.191539	0.004832	0.282221
-23.409167	-1.732307	3.201536	0.004802	0.282451
-23.333934	-1.701798	3.211533	0.004788	0.282677
-22.653036	-1.761776	3.221530	0.004661	0.283003
-22.402615	-1.772802	3.231526	0.004614	0.283179
-22.047679	-1.800802	3.241523	0.004548	0.283365
-21.826483	-1.793161	3.251520	0.004507	0.283610
-21.995343	-1.705715	3.261517	0.004539	0.283899
-22.023072	-1.650099	3.271514	0.004544	0.284156
-21.423314	-1.718145	3.281510	0.004432	0.284364
-21.071498	-1.743774	3.291507	0.004367	0.284559
-20.660005	-1.754319	3.301504	0.004290	0.284886
-20.340983	-1.774133	3.311501	0.004231	0.285079
-20.331070	-1.734168	3.321498	0.004229	0.285291
-19.745817	-1.793516	3.331494	0.004120	0.285529
-19.234513	-1.841972	3.341491	0.004025	0.285754
-19.341864	-1.790596	3.351488	0.004045	0.285915
-18.914425	-1.827370	3.361485	0.003966	0.286122
-18.786160	-1.794906	3.371482	0.003942	0.286404
-18.396832	-1.823717	3.381478	0.003870	0.286616
-18.423515	-1.779327	3.391475	0.003875	0.286815
-17.621522	-1.886004	3.401472	0.003725	0.287012
-17.513721	-1.853775	3.411469	0.003705	0.287273
-17.482974	-1.824771	3.421466	0.003700	0.287447
-17.203823	-1.833551	3.431462	0.003648	0.287658
-16.878477	-1.828676	3.441459	0.003587	0.287979
-17.216262	-1.731334	3.451456	0.003650	0.288159
-16.671334	-1.787784	3.461453	0.003549	0.288373
-15.924590	-1.879035	3.471450	0.003410	0.288596
-15.765803	-1.862064	3.481446	0.003380	0.288825
-15.213537	-1.932387	3.491443	0.003278	0.288976
-14.876659	-1.941447	3.501440	0.003215	0.289237
-14.860793	-1.903159	3.511437	0.003212	0.289442
-15.692813	-1.707125	3.521434	0.003367	0.289666
-15.052282	-1.778101	3.531430	0.003248	0.289892
-15.134589	-1.698982	3.541427	0.003263	0.290212
-14.942086	-1.680714	3.551424	0.003227	0.290477
-14.426548	-1.732189	3.561421	0.003132	0.290687
-14.341361	-1.709625	3.571418	0.003116	0.290876
-13.710991	-1.774762	3.581414	0.002998	0.291122
-13.411199	-1.774375	3.591411	0.002943	0.291394
-13.034536	-1.803469	3.601408	0.002873	0.291590
-12.527375	-1.857183	3.611405	0.002778	0.291780
-12.609290	-1.789158	3.621402	0.002794	0.292043
-12.193849	-1.817513	3.631398	0.002716	0.292277
-12.373989	-1.745574	3.641395	0.002750	0.292470
-11.605509	-1.841596	3.651392	0.002607	0.292686
-11.254510	-1.843758	3.661389	0.002542	0.292990
-11.365335	-1.787256	3.671386	0.002562	0.293169
-10.985955	-1.820484	3.681382	0.002492	0.293345
-11.083640	-1.742659	3.691379	0.002510	0.293641
-10.522450	-1.797616	3.701376	0.002406	0.293873
-10.141185	-1.825224	3.711373	0.002335	0.294078
-9.611469	-1.883468	3.721370	0.002236	0.294264
-9.365972	-1.875748	3.731366	0.002191	0.294521
-9.762811	-1.765537	3.741363	0.002264	0.294708
-9.279125	-1.811385	3.751360	0.002174	0.294914
-8.667481	-1.864695	3.761357	0.002061	0.295198
-8.185520	-1.917021	3.771354	0.001971	0.295370
-7.977229	-1.922003	3.781350	0.001932	0.295531
-7.993499	-1.869692	3.791347	0.001935	0.295772
-7.851792	-1.857552	3.801344	0.001909	0.295957
-7.309250	-1.923699	3.811341	0.001808	0.296115
-7.177369	-1.890249	3.821338	0.001784	0.296396
-6.695815	-1.937729	3.831334	0.001694	0.296591
-6.296156	-1.983933	3.841331	0.001620	0.296719
-6.860752	-1.818968	3.851328	0.001725	0.297023
-6.690330	-1.807073	3.861325	0.001693	0.297231
-6.763777	-1.746049	3.871322	0.001707	0.297463
-6.885033	-1.669603	3.881318	0.001729	0.297727
-5.746753	-1.817754	3.891315	0.001518	0.298012
-6.505201	-1.634461	3.901312	0.001659	0.298232
-6.140727	-1.645479	3.911309	0.001591	0.298500
-5.359460	-1.744006	3.921306	0.001446	0.298710
-6.034241	-1.567294	3.931302	0.001571	0.298972
-4.663774	-1.758456	3.941299	0.001316	0.299252
-4.817957	-1.680320	3.951296	0.001345	0.299493
-4.667732	-1.653604	3.961293	0.001317	0.299754
-4.903418	-1.559369	3.971290	0.001361	0.300002
-5.025276	-1.478866	3.981286	0.001384	0.300283
-5.031802	-1.411325	3.991283	0.001385	0.300602
-4.922172	-1.380522	4.001280	0.001365	0.300846
-4.748825	-1.346147	4.011277	0.001332	0.301162
-4.052855	-1.418331	4.021274	0.001203	0.301422
-4.005869	-1.360674	4.031270	0.001194	0.301740
-4.182925	-1.266918	4.041267	0.001227	0.302035
-3.558210	-1.314718	4.051264	0.001111	0.302349
-3.898639	-1.186185	4.061261	0.001174	0.302667
-3.828145	-1.122513	4.071258	0.001161	0.303033
-3.531118	-1.114059	4.081254	0.001106	0.303330
-3.363899	-1.074366	4.091251	0.001075	0.303664
-3.648223	-0.947838	4.101248	0.001128	0.304020
-3.034870	-0.986324	4.111245	0.001014	0.304367
-3.632749	-0.801351	4.121242	0.001125	0.304729
-2.849850	-0.867664	4.131238	0.000979	0.305089
-2.224240	-0.908747	4.141235	0.000863	0.305433
-2.184251	-0.852506	4.151232	0.000856	0.305733
-1.895337	-0.833548	4.161229	0.000802	0.306071
-2.345685	-0.672980	4.171226	0.000886	0.306443
-2.330277	-0.590628	4.181222	0.000883	0.306844
-2.139989	-0.551174	4.191219	0.000847	0.307193
-1.678643	-0.553905	4.201216	0.000762	0.307574
-1.341094	-0.529893	4.211213	0.000699	0.307975
-1.684714	-0.384151	4.221210	0.000763	0.308366
-1.198496	-0.391062	4.231206	0.000672	0.308747
-0.985198	-0.349070	4.241203	0.000633	0.309125
-1.223137	-0.222963	4.251200	0.000677	0.309512
-1.369072	-0.091808	4.261197	0.000704	0.310001
-1.086513	-0.054295	4.271194	0.000651	0.310415
-0.576588	-0.070427	4.281190	0.000557	0.310771
-0.016583	-0.081769	4.291187	0.000452	0.311191
0.650670	-0.127631	4.301184	0.000328	0.311541
0.527505	-0.020313	4.311181	0.000351	0.311935
0.330494	0.106045	4.321178	0.000388	0.312355
0.000000	0.268811	4.331174	0.000449	0.312830

0.268142	0.496523	4.336179	0.000399	0.314105
1.228371	0.881857	4.341184	0.000220	0.316673
2.056155	1.588561	4.346189	0.000066	0.320564
3.050192	2.565471	4.351194	-0.000120	0.325746
5.026993	3.662303	4.356198	-0.000489	0.332148
8.826179	4.737684	4.361203	-0.001197	0.339747
13.031947	6.077981	4.366208	-0.001981	0.348588
16.921845	7.810232	4.371213	-0.002706	0.358560
22.885357	9.511535	4.376218	-0.003818	0.369613
30.464443	11.300463	4.381222	-0.005230	0.381786
39.013702	13.315301	4.386227	-0.006823	0.395050
47.582180	15.729382	4.391232	-0.008420	0.409303
54.655719	18.833383	4.396237	-0.009739	0.424499
60.249490	22.624379	4.401242	-0.010783	0.440543
64.446724	27.057880	4.406246	-0.011568	0.457252
67.997541	31.998233	4.411251	-0.012232	0.474557
72.163204	37.212366	4.416256	-0.013011	0.492380
78.450360	42.444292	4.421261	-0.014185	0.510710
85.832519	47.874844	4.426266	-0.015563	0.529480
92.895293	53.775874	4.431270	-0.016882	0.548688
98.554925	60.317854	4.436275	-0.017940	0.568228
104.380517	67.195223	4.441280	-0.019029	0.588010
109.236097	74.569766	4.446285	-0.019938	0.607909
114.660816	82.176466	4.451290	-0.020953	0.627942
119.815981	90.123756	4.456294	-0.021918	0.648001
122.832888	98.736003	4.461299	-0.022485	0.668063
126.045217	107.510417	4.466304	-0.023089	0.687950
128.909382	116.546943	4.471309	-0.023628	0.707684
132.382466	125.657275	4.476314	-0.024281	0.727240
135.495115	134.995559	4.481318	-0.024867	0.746598
139.759835	144.255409	4.486323	-0.025667	0.765701
143.928696	153.683294	4.491328	-0.026449	0.784613
149.262699	162.996068	4.496333	-0.027448	0.803239
153.046566	172.703789	4.501338	-0.028159	0.821651
155.787073	182.650524	4.506342	-0.028676	0.839749
158.827376	192.557509	4.511347	-0.029248	0.857486
162.717819	202.335922	4.516352	-0.029979	0.874895
167.181157	212.031175	4.521357	-0.030817	0.891989
171.651592	221.756963	4.526362	-0.031655	0.908809
174.788797	231.695450	4.531366	-0.032246	0.925287
177.511663	241.682346	4.536371	-0.032759	0.941437
179.746947	251.708063	4.541376	-0.033182	0.957243
181.746412	261.717151	4.546381	-0.033561	0.972705
183.681574	271.673691	4.551386	-0.033928	0.987830
185.087482	281.625143	4.556390	-0.034196	1.002586
186.730946	291.445038	4.561395	-0.034508	1.017000
188.242281	301.223069	4.566400	-0.034796	1.031120
189.921939	310.866430	4.571405	-0.035115	1.044903
191.935924	320.394926	4.576410	-0.035496	1.058428
193.080644	330.006844	4.581414	-0.035715	1.071691
194.241325	339.519815	4.586419	-0.035938	1.084663
195.803602	348.889837	4.591424	-0.036235	1.097385
196.473311	358.339611	4.596429	-0.036366	1.109864
197.313271	367.673135	4.601434	-0.036528	1.122093
198.168386	376.935971	4.606438	-0.036693	1.134102
199.287289	386.075785	4.611443	-0.036908	1.145888
199.719014	395.311988	4.616448	-0.036994	1.157526
200.479742	404.359575	4.621453	-0.037141	1.168885
201.598845	413.304055	4.626458	-0.037356	1.180084
201.855662	422.358809	4.631462	-0.037409	1.191132
202.419233	431.279760	4.636467	-0.037520	1.201980
202.891820	440.196028	4.641472	-0.037614	1.212708
203.236502	449.057658	4.646477	-0.037684	1.223251
203.945088	457.837907	4.651482	-0.037821	1.233681
204.776817	466.510277	4.656486	-0.037982	1.243922
205.301653	475.244463	4.661491	-0.038085	1.254091
205.946180	483.902436	4.666496	-0.038211	1.264114
206.286479	492.593992	4.671501	-0.038280	1.274038
206.917708	501.192824	4.676506	-0.038403	1.283836
207.205175	509.832859	4.681510	-0.038462	1.293540
208.349477	518.280590	4.686515	-0.038681	1.303119
209.212706	526.860227	4.691520	-0.038847	1.312721
209.279831	535.474431	4.696525	-0.038865	1.322145
210.099086	543.912088	4.701530	-0.039023	1.331447
211.010876	552.319187	4.706534	-0.039198	1.340668
211.337386	560.837361	4.711539	-0.039264	1.349840
211.750205	569.307228	4.716544	-0.039347	1.358914
211.866331	577.806232	4.721549	-0.039374	1.367906
212.403089	586.232860	4.726554	-0.039479	1.376837
213.174770	594.587524	4.731558	-0.039628	1.385676
215.199768	602.743439	4.736563	-0.040011	1.394469
216.759739	610.987269	4.741568	-0.040307	1.403216
217.629177	619.365095	4.746573	-0.040474	1.411929
218.516332	627.725765	4.751578	-0.040644	1.420573
219.174624	636.122479	4.756582	-0.040772	1.429163
220.175734	644.433030	4.761587	-0.040964	1.437672
220.512127	652.859569	4.766592	-0.041032	1.446136
221.552735	661.127875	4.771597	-0.041231	1.454510
222.218092	669.497095	4.776602	-0.041361	1.462873
222.527876	677.917467	4.781606	-0.041424	1.471182
222.966932	686.267952	4.786611	-0.041511	1.479396
223.764493	694.537516	4.791616	-0.041665	1.487544
224.307806	702.842930	4.796621	-0.041772	1.495641
225.190470	711.098355	4.801626	-0.041941	1.503700
226.036458	719.353284	4.806630	-0.042104	1.511709
226.267962	727.698816	4.811635	-0.042153	1.519666
226.677144	736.032667	4.816640	-0.042234	1.527598
227.425243	744.268480	4.821645	-0.042379	1.535449
228.001544	752.535183	4.826650	-0.042491	1.543263
228.476740	760.818397	4.831654	-0.042585	1.551037
228.822820	769.096931	4.836659	-0.042655	1.558748
230.181231	777.203237	4.841664	-0.042913	1.566414
230.866066	785.456461	4.846669	-0.043046	1.574076
231.645652	793.674553	4.851674	-0.043197	1.581683
231.580776	802.053378	4.856678	-0.043190	1.589276
231.818536	810.344144	4.861683	-0.043240	1.596797
232.675083	818.505136	4.866688	-0.043404	1.604255
233.003640	826.767971	4.871693	-0.043471	1.611694
233.622317	834.993337	4.876698	-0.043591	1.619107
234.288474	843.186184	4.881702	-0.043721	1.626464
235.187550	851.367235	4.886707	-0.043893	1.633810
235.938700	859.543393	4.891712	-0.044039	1.641097
235.835843	867.867770	4.896717	-0.044025	1.648363
236.667804	876.009816	4.901722	-0.044185	1.655567
237.199828	884.202150	4.906726	-0.044289	1.662742
237.657985	892.413258	4.911731	-0.044380	1.669893
238.137176	900.632923	4.916736	-0.044475	1.677023
238.531585	908.808735	4.921741	-0.044553	1.684073
239.380503	916.963944	4.926746	-0.044717	1.691138
239.754991	925.195211	4.931750	-0.044792	1.698174
240.320203	933.343919	4.936755	-0.044902	1.705136
240.746848	941.576328	4.941760	-0.044987	1.712122
241.520680	949.687155	4.946765	-0.045136	1.719024
241.683867	957.943898	4.951770	-0.045172	1.725939
242.454707	966.071048	4.956774	-0.045321	1.732798
243.151208	974.209865	4.961779	-0.045456	1.739630
243.577910	982.410870	4.966784	-0.045541	1.746451
244.257811	990.554492	4.971789	-0.045673	1.753231
244.960285	998.708108	4.976794	-0.045809	1.759996
245.495183	1006.872852	4.981798	-0.045913	1.766722
245.782232	1015.108359	4.986803	-0.045972	1.773449
246.357026	1023.251561	4.991808	-0.046085	1.780112
246.708227	1031.429461	4.996813	-0.046155	1.786750
247.527206	1039.575536	5.001818	-0.046313	1.793395
248.404753	1047.665015	5.006822	-0.046482	1.799979
249.117558	1055.786225	5.011827	-0.046620	1.806542
249.846595	1063.940496	5.016832	-0.046761	1.813110
250.232000	1072.106716	5.021837	-0.046838	1.819622
250.408347	1080.346390	5.026842	-0.046876	1.826142
250.259728	1088.623679	5.031846	-0.046854	1.832629
250.509739	1096.767728	5.036851	-0.046905	1.839038
251.012357	1104.873319	5.041856	-0.047004	1.845424
251.416153	1113.024489	5.046861	-0.047085	1.851812
252.064066	1121.130420	5.051866	-0.047211	1.858172
252.791195	1129.193696	5.056870	-0.047351	1.864486
253.104310	1137.377240	5.061875	-0.047415	1.870822
253.936138	1145.459999	5.066880	-0.047575	1.877121
254.405412	1153.579027	5.071885	-0.047668	1.883383
255.154349	1161.684111	5.076890	-0.047812	1.889647
255.609928	1169.823393	5.081894	-0.047902	1.895881
255.720192	1178.013520	5.086899	-0.047928	1.902094
256.463232	1186.111832	5.091904	-0.048072	1.908290
256.494041	1194.315905	5.096909	-0.048083	1.914464
256.810590	1202.468807	5.101914	-0.048147	1.920612
256.829520	1210.653634	5.106918	-0.048156	1.926730
257.952924	1218.642190	5.111923	-0.048370	1.932808
258.382698	1226.796539	5.116928	-0.048456	1.938911
258.320180	1234.995428	5.121933	-0.048449	1.944973
259.114176	1243.063599	5.126938	-0.048602	1.951015
260.002946	1251.097761	5.131942	-0.048773	1.957023
260.475692	1259.205155	5.136947	-0.048866	1.963021
260.681203	1267.390673	5.141952	-0.048910	1.969028
261.471568	1275.433591	5.146957	-0.049062	1.974976
261.867244	1283.561768	5.151962	-0.049141	1.980926
262.441590	1291.653530	5.156966	-0.049253	1.986851
262.994692	1299.781562	5.161971	-0.049362	1.992781
263.563414	1307.900712	5.166976	-0.049473	1.998690
263.155860	1316.130609	5.171981	-0.049402	2.004556
264.218701	1324.139658	5.176986	-0.049605	2.010403
264.327046	1332.339281	5.181990	-0.049631	2.016268
264.677548	1340.424887	5.186995	-0.049701	2.022060
264.796584	1348.594004	5.192000	-0.049729	2.027870
265.049365	1356.710141	5.197005	-0.049781	2.033641
265.987255	1364.707256	5.202010	-0.049961	2.039382
266.639902	1372.755730	5.207014	-0.050088	2.045114
267.021981	1380.884081	5.212019	-0.050164	2.050857
268.105027	1388.906164	5.217024	-0.050371	2.056582
268.577672	1397.012636	5.222029	-0.050464	2.062287
269.010759	1405.155842	5.227034	-0.050550	2.067998
269.510484	1413.279733	5.232038	-0.050648	2.073686
269.909000	1421.367510	5.237043	-0.050728	2.079324
270.237464	1429.499574	5.242048	-0.050794	2.084969
270.158154	1437.683202	5.247053	-0.050785	2.090594
270.717914	1445.773014	5.252058	-0.050894	2.096203
271.066320	1453.858603	5.257062	-0.050964	2.101773
271.934682	1461.885172	5.262067	-0.051131	2.107340
272.346324	1470.055200	5.267072	-0.051213	2.112944
272.498989	1478.167154	5.272077	-0.051247	2.118468
273.287252	1486.174130	5.277082	-0.051399	2.123969
273.540276	1494.317951	5.282086	-0.051451	2.129496
274.135529	1502.357017	5.287091	-0.051567	2.134971
274.605818	1510.462860	5.292096	-0.051660	2.140465
274.667949	1518.595215	5.297101	-0.051677	2.145923
274.781820	1526.772695	5.302106	-0.051703	2.151403
275.049626	1534.840089	5.307110	-0.051758	2.156809
275.607601	1542.856082	5.312115	-0.051867	2.162196
275.950110	1550.979836	5.317120	-0.051936	2.167620
276.411505	1559.051751	5.322125	-0.052028	2.173007
277.253938	1567.068648	5.327130	-0.052190	2.178381
277.507160	1575.193230	5.332134	-0.052242	2.183756
277.794752	1583.303653	5.337139	-0.052301	2.189112
278.035971	1591.429551	5.342144	-0.052351	2.194461
278.547107	1599.444448	5.347149	-0.052451	2.199750
279.170969	1607.498275	5.352154	-0.052573	2.205061
279.255268	1615.637026	5.357158	-0.052594	2.210365
279.751698	1623.691689	5.362163	-0.052691	2.215639
280.540065	1631.721608	5.367168	-0.052843	2.220912
280.376362	1639.899981	5.372173	-0.052818	2.226181
280.586888	1648.015164	5.377178	-0.052863	2.231431
281.185802	1656.055943	5.382182	-0.052979	2.236655
281.518519	1664.125780	5.387187	-0.053047	2.241862
282.017067	1672.188964	5.392192	-0.053145	2.247068
282.210068	1680.296334	5.397197	-0.053186	2.252262
282.469867	1688.405637	5.402202	-0.053239	2.257452
282.894315	1696.449860	5.407206	-0.053324	2.262602
282.853533	1704.606359	5.412211	-0.053321	2.267771
283.718091	1712.634293	5.417216	-0.053488	2.272927
283.983570	1720.685316	5.422221	-0.053542	2.278032
283.540996	1728.890514	5.427226	-0.053465	2.283162
283.896504	1736.923266	5.432230	-0.053536	2.288241
284.221597	1744.978085	5.437235	-0.053602	2.293320
284.106532	1753.122528	5.442240	-0.053586	2.298406
284.316452	1761.163778	5.447245	-0.053630	2.303444
284.982554	1769.170506	5.452250	-0.053760	2.308489
285.317019	1777.234795	5.457254	-0.053827	2.313530
285.489424	1785.305658	5.462259	-0.053864	2.318550
285.683142	1793.395010	5.467264	-0.053906	2.323572
286.138491	1801.420384	5.472269	-0.053996	2.328567
286.846520	1809.454377	5.477274	-0.054133	2.333577
287.154778	1817.543435	5.482278	-0.054195	2.338576
287.441357	1825.598986	5.487283	-0.054254	2.343542
287.477981	1833.750783	5.492288	-0.054266	2.348536
287.970111	1841.791542	5.497293	-0.054363	2.353489
288.277702	1849.861822	5.502298	-0.054425	2.358435
288.824639	1857.857740	5.507302	-0.054532	2.363344
288.836258	1866.005412	5.512307	-0.054540	2.368292
289.251835	1874.061635	5.517312	-0.054622	2.373206
289.841700	1882.075659	5.522317	-0.054737	2.378099
289.974549	1890.182948	5.527322	-0.054767	2.383001
290.245374	1898.285870	5.532326	-0.054823	2.387902
290.559210	1906.353297	5.537331	-0.054887	2.392774
291.422659	1914.316216	5.542336	-0.055053	2.397618
291.565483	1922.388193	5.547341	-0.055085	2.402460
292.248991	1930.421757	5.552346	-0.055217	2.407312
292.714008	1938.521633	5.557350	-0.055309	2.412176
292.725028	1946.645928	5.562355	-0.055316	2.417009
293.460474	1954.660795	5.567360	-0.055458	2.421825
293.322742	1962.814305	5.572365	-0.055438	2.426644
293.642449	1970.903638	5.577370	-0.055503	2.431451
294.171814	1978.919964	5.582374	-0.055606	2.436223
294.718081	1986.927569	5.587379	-0.055713	2.440981
294.547448	1995.087419	5.592384	-0.055687	2.445763
294.625444	2003.162924	5.597389	-0.055707	2.450506
294.849833	2011.254589	5.602394	-0.055754	2.455261
295.628944	2019.196824	5.607398	-0.055904	2.459961
296.232546	2027.185598	5.612403	-0.056021	2.464667
296.594581	2035.292339	5.617408	-0.056094	2.469413
296.574338	2043.411487	5.622413	-0.056096	2.474128
297.533288	2051.349832	5.627418	-0.056279	2.478804
297.677021	2059.453755	5.632422	-0.056311	2.483504
297.532942	2067.616899	5.637427	-0.056290	2.488209
297.855016	2075.695671	5.642432	-0.056355	2.492891
298.054878	2083.721298	5.647437	-0.056397	2.497524
297.896349	2091.888750	5.652442	-0.056373	2.502203
298.260158	2099.900114	5.657446	-0.056446	2.506824
298.458632	2107.970564	5.662451	-0.056488	2.511457
298.645513	2116.037308	5.667456	-0.056528	2.516078
299.151182	2124.004696	5.672461	-0.056628	2.520658
299.593220	2132.023378	5.677466	-0.056715	2.525254
299.900158	2140.085617	5.682470	-0.056777	2.529856
300.275690	2148.130780	5.687475	-0.056853	2.534445
300.756884	2156.204820	5.692480	-0.056947	2.539050
300.694095	2164.293817	5.697485	-0.056941	2.543616
301.170187	2172.321194	5.702490	-0.057035	2.548177
301.219792	2180.439370	5.707494	-0.057049	2.552751
301.361686	2188.484752	5.712499	-0.057081	2.557282
302.154290	2196.464446	5.717504	-0.057234	2.561814
302.881809	2204.431049	5.722509	-0.057374	2.566327
303.137487	2212.557830	5.727514	-0.057427	2.570887
303.198562	2220.647421	5.732518	-0.057444	2.575405
302.810458	2228.829414	5.737523	-0.057377	2.579935
302.986734	2236.879515	5.742528	-0.057415	2.584423
303.104465	2244.927466	5.747533	-0.057442	2.588898
303.505054	2253.051931	5.752538	-0.057522	2.593428
303.721959	2261.080905	5.757542	-0.057567	2.597883
304.158059	2269.022152	5.762547	-0.057654	2.602298
304.474698	2277.059588	5.767552	-0.057718	2.606751
304.617733	2285.130990	5.772557	-0.057750	2.611202
305.133836	2293.148881	5.777562	-0.057851	2.615642
304.685415	2301.325835	5.782566	-0.057773	2.620095
304.830601	2309.321498	5.787571	-0.057805	2.624482
305.544798	2317.322183	5.792576	-0.057943	2.628903
305.766516	2325.383325	5.797581	-0.057990	2.633317
306.052596	2333.401680	5.802586	-0.058048	2.637704
306.462805	2341.419922	5.807590	-0.058130	2.642091
306.736058	2349.480184	5.812595	-0.058186	2.646485
307.756205	2357.434182	5.817600	-0.058381	2.650864
307.335912	2365.628489	5.822605	-0.058308	2.655270
307.878936	2373.634671	5.827610	-0.058414	2.659631
308.178877	2381.682438	5.832614	-0.058475	2.663991
308.785748	2389.695497	5.837619	-0.058594	2.668345
309.247573	2397.779298	5.842624	-0.058685	2.672721
309.292340	2405.842588	5.847629	-0.058698	2.677050
309.921874	2413.825455	5.852634	-0.058821	2.681368
310.044490	2421.907272	5.857638	-0.058849	2.685699
310.437106	2429.951823	5.862643	-0.058927	2.690021
310.267039	2438.107178	5.867648	-0.058901	2.694358
310.809232	2446.073598	5.872653	-0.059007	2.698633
310.979828	2454.137344	5.877658	-0.059044	2.702930
311.356562	2462.176164	5.882662	-0.059119	2.707220
311.433035	2470.267726	5.887667	-0.059139	2.711511
311.411143	2478.394051	5.892672	-0.059140	2.715808
311.731943	2486.357726	5.897677	-0.059205	2.720034
312.273207	2494.335361	5.902682	-0.059311	2.724274
312.175009	2502.473616	5.907686	-0.059298	2.728553
312.185416	2510.563450	5.912691	-0.059305	2.732805
313.186933	2518.480809	5.917696	-0.059496	2.737023
312.885861	2526.602707	5.922701	-0.059446	2.741260
313.658980	2534.572660	5.927706	-0.059595	2.745478
314.135500	2542.604938	5.932710	-0.059689	2.749703
314.189005	2550.768953	5.937715	-0.059704	2.753964
315.272954	2558.653156	5.942720	-0.059911	2.758137
315.571754	2566.697486	5.947725	-0.059972	2.762338
315.931221	2574.759113	5.952730	-0.060044	2.766545
316.199798	2582.845750	5.957734	-0.060099	2.770753
316.138144	2590.947493	5.962739	-0.060093	2.774943
316.846656	2598.910492	5.967744	-0.060230	2.779101
316.763879	2606.999243	5.972749	-0.060220	2.783270
316.862844	2615.117001	5.977754	-0.060243	2.787458
317.158572	2623.170584	5.982758	-0.060304	2.791619
317.180272	2631.230026	5.987763	-0.060313	2.795761
317.933962	2639.197258	5.992768	-0.060458	2.799892
317.746649	2647.264811	5.997773	-0.060429	2.804013
317.593789	2655.369457	6.002778	-0.060406	2.808149
318.648371	2663.282958	6.007782	-0.060607	2.812252
318.618248	2671.388090	6.012787	-0.060607	2.816383
319.291184	2679.380920	6.017792	-0.060737	2.820492
319.389195	2687.441665	6.022797	-0.060761	2.824596
319.881970	2695.492736	6.027802	-0.060858	2.828712
320.066887	2703.559161	6.032806	-0.060897	2.832812
320.064502	2711.613823	6.037811	-0.060902	2.836889
320.691487	2719.613532	6.042816	-0.061024	2.840969
321.645605	2727.517734	6.047821	-0.061207	2.845014
321.960991	2735.599015	6.052826	-0.061271	2.849105
322.108596	2743.689491	6.057830	-0.061303	2.853185
322.622139	2751.712699	6.062835	-0.061404	2.857246
322.863291	2759.820268	6.067840	-0.061454	2.861329
323.039568	2767.855265	6.072845	-0.061492	2.865365
323.558211	2775.881048	6.077850	-0.061594	2.869410
323.895095	2783.957747	6.082854	-0.061662	2.873465
324.083378	2791.968269	6.087859	-0.061702	2.877473
324.490227	2800.040695	6.092864	-0.061783	2.881518
325.034069	2808.022650	6.097869	-0.061890	2.885520
324.964699	2816.150824	6.102874	-0.061882	2.889555
325.238285	2824.205947	6.107878	-0.061938	2.893567
325.755446	2832.183379	6.112883	-0.062040	2.897549
326.126519	2840.245206	6.117888	-0.062114	2.901558
326.687770	2848.223227	6.122893	-0.062224	2.905531
326.497101	2856.381596	6.127898	-0.062194	2.909547
326.650135	2864.507901	6.132902	-0.062227	2.913559
327.024977	2872.458386	6.137907	-0.062302	2.917492
327.479987	2880.468153	6.142912	-0.062392	2.921453
328.073118	2888.394848	6.147917	-0.062508	2.925375
328.256418	2896.466941	6.152922	-0.062547	2.929341
328.496186	2904.550887	6.157926	-0.062597	2.933310
329.103092	2912.523766	6.162931	-0.062715	2.937240
329.419908	2920.615638	6.167936	-0.062779	2.941206
329.704225	2928.628593	6.172941	-0.062837	2.945127
330.080523	2936.679559	6.177946	-0.062913	2.949066
330.742082	2944.696888	6.182950	-0.063041	2.952999
330.886576	2952.748104	6.187955	-0.063073	2.956915
330.985684	2960.847231	6.192960	-0.063097	2.960847
331.483073	2968.807509	6.197965	-0.063195	2.964727
331.466356	2976.929787	6.202970	-0.063197	2.968654
332.241971	2984.890473	6.207974	-0.063346	2.972538
332.442797	2992.984910	6.212979	-0.063389	2.976452
332.700483	3001.024316	6.217984	-0.063442	2.980338
333.173786	3009.002464	6.222989	-0.063536	2.984200
333.284297	3017.114683	6.227994	-0.063561	2.988102
333.745157	3025.152507	6.232998	-0.063652	2.991982
333.810250	3033.179433	6.238003	-0.063670	2.995831
333.847208	3041.251065	6.243008	-0.063682	2.999695
334.275321	3049.235893	6.248013	-0.063767	3.003533
334.820743	3057.245528	6.253018	-0.063873	3.007383
335.135414	3065.291528	6.258022	-0.063937	3.011234
335.385951	3073.360045	6.263027	-0.063989	3.015087
335.802495	3081.379415	6.268032	-0.064072	3.018921
335.741982	3089.447059	6.273037	-0.064066	3.022749
335.988011	3097.486019	6.278042	-0.064117	3.026573
335.830654	3105.595515	6.283046	-0.064093	3.030406
336.253065	3113.570469	6.288051	-0.064177	3.034199
336.836347	3121.556629	6.293056	-0.064290	3.038001
336.942913	3129.620836	6.298061	-0.064315	3.041811
337.232397	3137.662201	6.303066	-0.064375	3.045614
337.459096	3145.692440	6.308070	-0.064422	3.049405
337.723067	3153.717621	6.313075	-0.064476	3.053190
338.277209	3161.743415	6.318080	-0.064585	3.056985
338.488210	3169.767723	6.323085	-0.064629	3.060757
338.792988	3177.803023	6.328090	-0.064691	3.064535
339.152268	3185.873504	6.333094	-0.064763	3.068327
339.704566	3193.879441	6.338099	-0.064871	3.072093
339.541756	3202.027275	6.343104	-0.064846	3.075887
339.726245	3209.999281	6.348109	-0.064886	3.079611
340.107072	3217.991131	6.353114	-0.064962	3.083348
340.387615	3226.049503	6.358118	-0.065019	3.087107
340.367339	3234.110865	6.363123	-0.065021	3.090849
341.395696	3242.054316	6.368128	-0.065217	3.094581
341.991490	3250.043765	6.373133	-0.065333	3.098309
342.362403	3258.076094	6.378138	-0.065408	3.102042
342.898038	3266.119875	6.383142	-0.065513	3.105784
343.107432	3274.176819	6.388147	-0.065557	3.109512
343.487167	3282.263644	6.393152	-0.065633	3.113256
343.379602	3290.323957	6.398157	-0.065618	3.116962
343.822283	3298.353480	6.403162	-0.065706	3.120674
344.012510	3306.354850	6.408166	-0.065746	3.124358
343.870195	3314.433097	6.413171	-0.065725	3.128057
344.841918	3322.404799	6.418176	-0.065911	3.131753
345.291689	3330.437087	6.423181	-0.066000	3.135449
345.439297	3338.474293	6.428186	-0.066033	3.139130
345.610130	3346.515286	6.433190	-0.066070	3.142808
345.764552	3354.589342	6.438195	-0.066104	3.146497
346.185816	3362.622563	6.443200	-0.066187	3.150175
346.310496	3370.676125	6.448205	-0.066216	3.153844
346.214062	3378.759543	6.453210	-0.066203	3.157513
346.678581	3386.740045	6.458214	-0.066295	3.161155
346.988527	3394.721041	6.463219	-0.066358	3.164787
347.891132	3402.687139	6.468224	-0.066531	3.168434
347.834506	3410.782172	6.473229	-0.066525	3.172093
347.856320	3418.898934	6.478234	-0.066535	3.175761
348.171078	3426.927356	6.483238	-0.066599	3.179397
348.586928	3434.867987	6.488243	-0.066681	3.182994
348.738107	3442.970451	6.493248	-0.066715	3.186649
348.740871	3451.020938	6.498253	-0.066720	3.190269
348.849648	3459.074516	6.503258	-0.066746	3.193891
349.337705	3467.036697	6.508262	-0.066842	3.197485
349.435043	3475.095147	6.513267	-0.066865	3.201100
349.960924	3483.058833	6.518272	-0.066968	3.204688
350.521592	3491.061215	6.523277	-0.067078	3.208290
350.584302	3499.185514	6.528282	-0.067095	3.211921
351.193348	3507.175912	6.533286	-0.067213	3.215512
351.420934	3515.192232	6.538291	-0.067261	3.219094
352.089429	3523.158877	6.543296	-0.067391	3.222668
351.677969	3531.322084	6.548301	-0.067319	3.226280
351.936838	3539.375268	6.553306	-0.067373	3.229868
351.964079	3547.423496	6.558310	-0.067383	3.233439
352.477609	3555.375621	6.563315	-0.067484	3.236984
353.391642	3563.347767	6.568320	-0.067659	3.240551
354.055860	3571.271346	6.573325	-0.067788	3.244082
353.682606	3579.454490	6.578330	-0.067724	3.247681
354.215934	3587.461299	6.583334	-0.067828	3.251235
354.743700	3595.470570	6.588339	-0.067932	3.254787
354.488855	3603.603526	6.593344	-0.067889	3.258356
354.692166	3611.601878	6.598349	-0.067932	3.261882
355.182678	3619.595895	6.603354	-0.068029	3.265413
355.476763	3627.632634	6.608358	-0.068089	3.268951
355.479992	3635.722166	6.613363	-0.068095	3.272497
356.669595	3643.629940	6.618368	-0.068321	3.276007
356.863744	3651.671075	6.623373	-0.068363	3.279531
357.007548	3659.724862	6.628378	-0.068395	3.283056
356.512765	3667.891596	6.633382	-0.068308	3.286600
356.726024	3675.891939	6.638387	-0.068353	3.290096
357.138581	3683.897816	6.643392	-0.068435	3.293598
357.008108	3691.961053	6.648397	-0.068416	3.297101
357.856783	3699.908793	6.653402	-0.068579	3.300587
358.274602	3707.900745	6.658406	-0.068662	3.304073
358.663737	3715.929150	6.663411	-0.068739	3.307569
359.097953	3724.011947	6.668416	-0.068826	3.311087
359.126959	3732.064903	6.673421	-0.068836	3.314572
359.538767	3740.037816	6.678426	-0.068918	3.318034
359.784806	3748.096317	6.683430	-0.068969	3.321523
360.246080	3756.068151	6.688435	-0.069060	3.324979
360.690672	3764.135545	6.693440	-0.069148	3.328472
360.515440	3772.224654	6.698445	-0.069121	3.331947
360.839300	3780.234985	6.703450	-0.069186	3.335403
361.551390	3788.201238	6.708454	-0.069324	3.338852
361.686507	3796.244515	6.713459	-0.069354	3.342308
361.688205	3804.374996	6.718464	-0.069360	3.345793
362.354168	3812.308908	6.723469	-0.069489	3.349215
362.567665	3820.353768	6.728474	-0.069534	3.352664
362.980277	3828.396169	6.733478	-0.069616	3.356115
363.276789	3836.383282	6.738483	-0.069676	3.359536
363.578811	3844.412634	6.743488	-0.069738	3.362970
363.805758	3852.454676	6.748493	-0.069785	3.366404
364.226496	3860.480890	6.753498	-0.069869	3.369835
364.948562	3868.456341	6.758502	-0.070008	3.373252
364.492790	3876.600071	6.763507	-0.069929	3.376693
364.878359	3884.621961	6.768512	-0.070006	3.380110
365.418882	3892.579134	6.773517	-0.070112	3.383502
365.267994	3900.704212	6.778522	-0.070089	3.386936
366.000672	3908.686514	6.783526	-0.070230	3.390338
366.582061	3916.689371	6.788531	-0.070344	3.393741
366.982500	3924.729280	6.793536	-0.070424	3.397148
366.271501	3932.888969	6.798541	-0.070296	3.400563
366.171476	3940.853437	6.803546	-0.070283	3.403914
366.829098	3948.849941	6.808550	-0.070411	3.407303
366.813756	3956.893699	6.813555	-0.070413	3.410683
367.298170	3964.893679	6.818560	-0.070508	3.414060
367.701426	3972.892256	6.823565	-0.070589	3.417430
367.754227	3980.950662	6.828570	-0.070604	3.420809
367.843866	3988.978179	6.833574	-0.070626	3.424174
368.808655	3996.902535	6.838579	-0.070810	3.427522
369.085116	4005.004525	6.843584	-0.070867	3.430917
369.094556	4013.018631	6.848589	-0.070874	3.434263
369.734193	4021.004081	6.853594	-0.070998	3.437615
370.598103	4029.030079	6.858598	-0.071164	3.440989
370.520575	4037.078959	6.863603	-0.071155	3.444336
370.831070	4045.120246	6.868608	-0.071218	3.447691
371.099875	4053.193993	6.873613	-0.071273	3.451054
371.786907	4061.111300	6.878618	-0.071406	3.454363
371.681992	4069.267707	6.883622	-0.071392	3.457741
372.428584	4077.204303	6.888627	-0.071536	3.461053
373.194175	4085.206949	6.893632	-0.071684	3.464390
373.026425	4093.284289	6.898637	-0.071658	3.467724
373.495049	4101.311804	6.903642	-0.071751	3.471054
373.618080	4109.402397	6.908646	-0.071779	3.474397
374.135116	4117.325907	6.913651	-0.071880	3.477680
374.315983	4125.434333	6.918656	-0.071919	3.481025
374.588239	4133.352757	6.923661	-0.071975	3.484291
375.117717	4141.404104	6.928666	-0.072079	3.487618
375.514179	4149.487690	6.933670	-0.072158	3.490950
375.950265	4157.425276	6.938675	-0.072244	3.494220
375.659972	4165.618663	6.943680	-0.072195	3.497568
376.260486	4173.561620	6.948685	-0.072312	3.500840
376.445130	4181.556569	6.953690	-0.072352	3.504116
376.905786	4189.600036	6.958694	-0.072443	3.507418
377.201073	4197.645166	6.963699	-0.072503	3.510712
377.532071	4205.674523	6.968704	-0.072570	3.513998
377.512702	4213.753498	6.973709	-0.072571	3.517289
377.921161	4221.717693	6.978714	-0.072653	3.520544
378.529086	4229.661658	6.983718	-0.072771	3.523795
378.420633	4237.773343	6.988723	-0.072756	3.527088
379.566489	4245.747061	6.993728	-0.072975	3.530361
379.856518	4253.812469	6.998733	-0.073034	3.533641
380.591245	4261.785766	7.003738	-0.073176	3.536895
381.170739	4269.798729	7.008742	-0.073289	3.540157
381.531877	4277.802098	7.013747	-0.073361	3.543405
381.562973	4285.954139	7.018752	-0.073372	3.546700
381.564958	4294.010003	7.023757	-0.073378	3.549952
382.178514	4302.014402	7.028762	-0.073497	3.553199
382.014859	4310.111669	7.033766	-0.073472	3.556457
382.786181	4317.966397	7.038771	-0.073621	3.559643
382.918849	4326.050619	7.043776	-0.073651	3.562898
383.254502	4334.074962	7.048781	-0.073718	3.566133
383.284381	4342.095455	7.053786	-0.073729	3.569354
383.945290	4350.111048	7.058790	-0.073857	3.572589
384.369219	4358.123840	7.063795	-0.073942	3.575813
384.088184	4366.201986	7.068800	-0.073895	3.579039
384.729245	4374.177477	7.073805	-0.074019	3.582248
385.340355	4382.147006	7.078810	-0.074138	3.585451
385.770818	4390.209252	7.083814	-0.074223	3.588683
385.528858	4398.328482	7.088819	-0.074184	3.591915
385.765298	4406.360231	7.093824	-0.074233	3.595123
385.989840	4414.340531	7.098829	-0.074280	3.598308
386.650786	4422.300841	7.103834	-0.074408	3.601494
386.825998	4430.340825	7.108838	-0.074446	3.604695
387.296946	4438.340603	7.113843	-0.074539	3.607886
387.741909	4446.414114	7.118848	-0.074627	3.611102
387.746954	4454.471672	7.123853	-0.074633	3.614296
388.622597	4462.423948	7.128858	-0.074801	3.617471
388.360312	4470.564055	7.133862	-0.074758	3.620685
388.350732	4478.548606	7.138867	-0.074761	3.623842
388.809124	4486.580202	7.143872	-0.074851	3.627027
388.943947	4494.617608	7.148877	-0.074882	3.630203
389.402691	4502.578897	7.153882	-0.074972	3.633356
389.780534	4510.629946	7.158886	-0.075048	3.636538
389.829232	4518.648020	7.163891	-0.075062	3.639696
390.422826	4526.621963	7.168896	-0.075178	3.642848
390.223598	4534.740697	7.173901	-0.075146	3.646033
391.165461	4542.628133	7.178906	-0.075327	3.649156
391.593906	4550.697992	7.183910	-0.075412	3.652333
391.446037	4558.791349	7.188915	-0.075389	3.655501
392.350434	4566.739548	7.193920	-0.075563	3.658638
392.199716	4574.845566	7.198925	-0.075540	3.661805
392.636067	4582.812488	7.203930	-0.075626	3.664931
393.232428	4590.841760	7.208934	-0.075743	3.668083
393.251610	4598.894677	7.213939	-0.075751	3.671226
393.363458	4606.946556	7.218944	-0.075777	3.674368
393.565743	4614.946287	7.223949	-0.075820	3.677490
393.750114	4622.996664	7.228954	-0.075860	3.680628
393.964461	4631.000563	7.233958	-0.075905	3.683747
394.326251	4638.967595	7.238963	-0.075977	3.686852
394.996089	4646.999543	7.243968	-0.076107	3.689987
395.488752	4655.015137	7.248973	-0.076204	3.693109
395.582390	4663.090334	7.253978	-0.076227	3.696241
396.255568	4671.051342	7.258982	-0.076357	3.699342
396.628594	4679.078937	7.263987	-0.076432	3.702457
396.907789	4687.163345	7.268992	-0.076489	3.705589
397.390384	4695.158741	7.273997	-0.076584	3.708690
397.336307	4703.281551	7.279002	-0.076580	3.711823
397.550835	4711.331111	7.284006	-0.076625	3.714932
397.667984	4719.298260	7.289011	-0.076652	3.718005
398.268928	4727.260604	7.294016	-0.076769	3.721085
398.896048	4735.169639	7.299021	-0.076891	3.724142
398.866977	4743.281045	7.304026	-0.076890	3.727259
399.190986	4751.308764	7.309030	-0.076956	3.730349
399.653469	4759.301751	7.314035	-0.077047	3.733427
400.032122	4767.390889	7.319040	-0.077123	3.736537
400.253053	4775.392722	7.324045	-0.077169	3.739608
400.311452	4783.445954	7.329050	-0.077185	3.742691
400.568620	4791.468627	7.334054	-0.077238	3.745765
400.950284	4799.438561	7.339059	-0.077315	3.748819
401.741321	4807.476663	7.344064	-0.077467	3.751907
401.889189	4815.506868	7.349069	-0.077500	3.754973
401.766581	4823.546065	7.354074	-0.077482	3.758034
401.927553	4831.612439	7.359078	-0.077518	3.761109
402.021195	4839.544430	7.364083	-0.077540	3.764130
402.370131	4847.658261	7.369088	-0.077610	3.767223
402.715889	4855.617143	7.374093	-0.077680	3.770254
403.339701	4863.610532	7.379098	-0.077801	3.773303
403.865377	4871.655470	7.384102	-0.077904	3.776366
404.358387	4879.609467	7.389107	-0.078001	3.779392
404.814363	4887.680410	7.394112	-0.078091	3.782458
405.158297	4895.703906	7.399117	-0.078161	3.785501
405.383589	4903.761946	7.404122	-0.078208	3.788552
405.622798	4911.825739	7.409126	-0.078258	3.791604
405.878049	4919.804953	7.414131	-0.078310	3.794621
406.672481	4927.786069	7.419136	-0.078463	3.797648
406.464860	4935.914948	7.424141	-0.078430	3.800706
406.809027	4943.864362	7.429146	-0.078499	3.803707
407.344554	4951.886754	7.434150	-0.078604	3.806737
407.799020	4959.835049	7.439155	-0.078694	3.809735
407.837085	4967.949398	7.444160	-0.078706	3.812783
408.326267	4975.979327	7.449165	-0.078802	3.815807
408.822489	4983.943798	7.454170	-0.078900	3.818805
409.018285	4992.038383	7.459174	-0.078942	3.821842
408.955582	5000.035434	7.464179	-0.078935	3.824834
409.290588	5008.124742	7.469184	-0.079003	3.827868
409.041049	5016.193843	7.474189	-0.078962	3.830878
409.602638	5024.098096	7.479194	-0.079071	3.833842
410.067858	5032.154922	7.484198	-0.079163	3.836859
410.393123	5040.100774	7.489203	-0.079229	3.839829
410.871166	5048.117028	7.494208	-0.079323	3.842826
411.045636	5056.181559	7.499213	-0.079361	3.845832
411.327138	5064.175821	7.504218	-0.079418	3.848812
411.585833	5072.293661	7.509222	-0.079472	3.851835
411.671760	5080.266395	7.514227	-0.079493	3.854799
412.076371	5088.297058	7.519232	-0.079573	3.857788
411.996555	5096.355650	7.524237	-0.079564	3.860774
411.790440	5104.368580	7.529242	-0.079531	3.863739
412.813280	5112.301645	7.534246	-0.079726	3.866698
412.907385	5120.355716	7.539251	-0.079749	3.869680
413.706154	5128.429948	7.544256	-0.079903	3.872681
413.824708	5136.512269	7.549261	-0.079930	3.875669
414.182845	5144.422616	7.554266	-0.080002	3.878597
414.610976	5152.469871	7.559270	-0.080087	3.881573
414.389455	5160.445687	7.564275	-0.080051	3.884508
415.267537	5168.419738	7.569280	-0.080219	3.887463
415.175257	5176.528790	7.574285	-0.080208	3.890445
414.731784	5184.601993	7.579290	-0.080130	3.893405
415.005898	5192.663484	7.584294	-0.080186	3.896372
415.669059	5200.522222	7.589299	-0.080315	3.899271
415.740975	5208.628360	7.594304	-0.080334	3.902246
416.545940	5216.489252	7.599309	-0.080489	3.905143
416.345188	5224.624103	7.604314	-0.080457	3.908119
416.578293	5232.718077	7.609318	-0.080505	3.911086
416.811248	5240.644967	7.614323	-0.080554	3.913990
417.481598	5248.680346	7.619328	-0.080684	3.916940
418.039124	5256.607436	7.624333	-0.080793	3.919845
418.078371	5264.661140	7.629338	-0.080805	3.922785
418.472656	5272.722904	7.634342	-0.080884	3.925732
418.724403	5280.737469	7.639347	-0.080936	3.928657
418.979602	5288.821421	7.644352	-0.080989	3.931605
419.482641	5296.799167	7.649357	-0.081087	3.934517
420.000353	5304.814076	7.654362	-0.081189	3.937441
420.404912	5312.844416	7.659366	-0.081270	3.940365
420.672660	5320.831108	7.664371	-0.081325	3.943270
421.072657	5328.907486	7.669376	-0.081404	3.946206
421.285419	5336.959917	7.674381	-0.081449	3.949129
421.184509	5345.027358	7.679386	-0.081436	3.952049
421.338601	5353.038710	7.684390	-0.081469	3.954951
421.441299	5361.010234	7.689395	-0.081494	3.957836
422.120991	5369.003755	7.694400	-0.081625	3.960737
422.389864	5376.983216	7.699405	-0.081681	3.963623
422.602068	5385.023354	7.704410	-0.081725	3.966528
423.216167	5393.007211	7.709414	-0.081845	3.969418
423.030533	5401.149143	7.714419	-0.081816	3.972348
423.462864	5409.134049	7.719424	-0.081901	3.975231
423.485414	5417.130162	7.724429	-0.081911	3.978108
423.410514	5425.214128	7.729434	-0.081902	3.981013
424.090889	5433.124874	7.734438	-0.082034	3.983867
424.434007	5441.157010	7.739443	-0.082103	3.986756
424.673309	5449.201848	7.744448	-0.082153	3.989646
425.051368	5457.228574	7.749453	-0.082228	3.992530
424.776044	5465.299335	7.754458	-0.082182	3.995416
424.784704	5473.296928	7.759462	-0.082189	3.998279
425.110345	5481.300148	7.764467	-0.082255	4.001147
425.735994	5489.240109	7.769472	-0.082376	4.003996
426.061958	5497.315443	7.774477	-0.082442	4.006886
425.854845	5505.381344	7.779482	-0.082409	4.009761
426.324256	5513.416304	7.784486	-0.082502	4.012635
426.491180	5521.406362	7.789491	-0.082538	4.015485
426.375865	5529.465148	7.794496	-0.082522	4.018353
426.467486	5537.472780	7.799501	-0.082544	4.021204
427.336076	5545.344429	7.804506	-0.082711	4.024018
427.585319	5553.482984	7.809510	-0.082762	4.026914
427.977439	5561.422293	7.814515	-0.082841	4.029740
428.696941	5569.471414	7.819520	-0.082980	4.032608
428.733852	5577.601220	7.824525	-0.082992	4.035491
428.867387	5585.550112	7.829530	-0.083022	4.038310
429.291530	5593.606360	7.834534	-0.083106	4.041170
429.410355	5601.551386	7.839539	-0.083133	4.043983
430.112182	5609.598201	7.844544	-0.083269	4.046839
430.249745	5617.623606	7.849549	-0.083300	4.049677
430.989462	5625.570923	7.854554	-0.083443	4.052495
431.337259	5633.665926	7.859558	-0.083513	4.055356
431.426137	5641.693859	7.864563	-0.083535	4.058188
431.725149	5649.744984	7.869568	-0.083596	4.061030
432.026632	5657.704206	7.874573	-0.083657	4.063837
432.262454	5665.755302	7.879578	-0.083706	4.066673
432.458451	5673.777400	7.884582	-0.083748	4.069497
432.518594	5681.856237	7.889587	-0.083764	4.072336
433.235339	5689.825046	7.894592	-0.083903	4.075145
433.410948	5697.833905	7.899597	-0.083941	4.077957
434.067665	5705.797135	7.904602	-0.084068	4.080759
434.324099	5713.842455	7.909606	-0.084121	4.083581
433.943511	5721.942964	7.914611	-0.084055	4.086412
434.217699	5729.915797	7.919616	-0.084112	4.089206
434.991421	5737.893413	7.924621	-0.084261	4.092006
434.964593	5745.910322	7.929626	-0.084261	4.094807
435.061431	5753.999259	7.934630	-0.084284	4.097633
435.811089	5761.935922	7.939635	-0.084429	4.100412
435.652778	5770.003408	7.944640	-0.084405	4.103223
435.841095	5778.049076	7.949645	-0.084445	4.106029
436.598406	5785.999688	7.954650	-0.084591	4.108808
437.066217	5794.072468	7.959654	-0.084683	4.111624
436.928666	5802.076907	7.964659	-0.084663	4.114405
437.556656	5810.089092	7.969664	-0.084785	4.117198
437.399931	5818.137559	7.974669	-0.084761	4.119990
437.891136	5826.083512	7.979674	-0.084858	4.122754
438.381726	5834.115186	7.984678	-0.084954	4.125546
438.851118	5842.095648	7.989683	-0.085047	4.128318
438.873831	5850.254749	7.994688	-0.085056	4.131143
438.979843	5858.237600	7.999693	-0.085081	4.133907
439.580074	5866.201752	8.004698	-0.085198	4.136669
440.260789	5874.210030	8.009702	-0.085330	4.139446
440.137641	5882.261266	8.014707	-0.085312	4.142224
440.448074	5890.252872	8.019712	-0.085375	4.144987
440.444684	5898.324943	8.024717	-0.085380	4.147770
440.725062	5906.325851	8.029722	-0.085437	4.150532
440.870440	5914.378863	8.034726	-0.085470	4.153307
441.370521	5922.333677	8.039731	-0.085568	4.156051
442.389447	5930.239761	8.044736	-0.085763	4.158783
442.008053	5938.450867	8.049741	-0.085697	4.161601
442.209605	5946.352830	8.054746	-0.085740	4.164318
442.481591	5954.475886	8.059750	-0.085796	4.167109
442.792774	5962.432873	8.064755	-0.085859	4.169843
443.001738	5970.478078	8.069760	-0.085903	4.172603
443.562456	5978.473531	8.074765	-0.086012	4.175349
443.950811	5986.507861	8.079770	-0.086090	4.178104
443.527596	5994.631466	8.084774	-0.086016	4.180878
444.109570	6002.497303	8.089779	-0.086130	4.183574
444.468720	6010.597295	8.094784	-0.086202	4.186346
444.322364	6018.662406	8.099789	-0.086180	4.189098
444.501265	6026.688802	8.104794	-0.086218	4.191839
445.568321	6034.631097	8.109798	-0.086422	4.194560
445.709422	6042.678727	8.114803	-0.086454	4.197303
446.014411	6050.639112	8.119808	-0.086516	4.200018
446.163747	6058.684261	8.124813	-0.086549	4.202757
446.313536	6066.689717	8.129818	-0.086582	4.205482
446.418367	6074.740496	8.134822	-0.086607	4.208219
446.756460	6082.733818	8.139827	-0.086675	4.210938
446.873251	6090.781005	8.144832	-0.086702	4.213670
446.741240	6098.879207	8.149837	-0.086682	4.216416
446.833601	6106.825310	8.154842	-0.086705	4.219110
448.273730	6114.765140	8.159846	-0.086978	4.221816
448.640370	6122.686377	8.164851	-0.087051	4.224501
448.572500	6130.842426	8.169856	-0.087044	4.227260
449.227701	6138.879671	8.174861	-0.087171	4.229984
449.709159	6146.855651	8.179866	-0.087266	4.232684
450.060712	6154.895491	8.184870	-0.087337	4.235402
450.147355	6162.903386	8.189875	-0.087358	4.238105
450.321750	6170.989716	8.194880	-0.087396	4.240834
451.179908	6178.854993	8.199885	-0.087561	4.243493
451.239044	6186.967405	8.204890	-0.087577	4.246226
451.363268	6194.986636	8.209894	-0.087605	4.248926
451.397971	6203.028529	8.214899	-0.087617	4.251631
451.772558	6211.044217	8.219904	-0.087692	4.254329
452.020687	6219.037233	8.224909	-0.087743	4.257017
451.711619	6227.108296	8.229914	-0.087691	4.259723
452.019155	6235.089369	8.234918	-0.087753	4.262404
452.323577	6243.046813	8.239923	-0.087815	4.265075
452.832279	6251.128475	8.244928	-0.087915	4.267787
453.076682	6259.138071	8.249933	-0.087966	4.270472
453.364898	6267.145056	8.254938	-0.088025	4.273154
453.411707	6275.216201	8.259942	-0.088039	4.275853
453.623750	6283.115042	8.264947	-0.088083	4.278495
453.637311	6291.209431	8.269952	-0.088091	4.281199
454.093137	6299.143477	8.274957	-0.088181	4.283851
454.339839	6307.214668	8.279962	-0.088232	4.286546
454.751023	6315.193893	8.284966	-0.088314	4.289210
455.281761	6323.206941	8.289971	-0.088418	4.291884
455.602535	6331.253271	8.294976	-0.088483	4.294566
456.109633	6339.298945	8.299981	-0.088582	4.297247
455.573588	6347.368557	8.304986	-0.088488	4.299926
455.715118	6355.398234	8.309990	-0.088519	4.302596
456.001097	6363.325821	8.314995	-0.088578	4.305231
456.031146	6371.424858	8.320000	-0.088589	4.307919
456.067049	6379.468569	8.325005	-0.088600	4.310588
456.212228	6387.428818	8.330010	-0.088633	4.313228
457.017000	6395.397408	8.335014	-0.088788	4.315874
457.009810	6403.372384	8.340019	-0.088791	4.318514
457.456600	6411.462894	8.345024	-0.088880	4.321195
457.136662	6419.465782	8.350029	-0.088825	4.323839
457.625079	6427.474774	8.355034	-0.088922	4.326489
458.280576	6435.442340	8.360038	-0.089049	4.329126
458.501645	6443.486828	8.365043	-0.089095	4.331783
459.057728	6451.474517	8.370048	-0.089204	4.334422
459.516728	6459.519780	8.375053	-0.089295	4.337077
459.702869	6467.543290	8.380058	-0.089334	4.339722
459.427791	6475.648737	8.385062	-0.089288	4.342388
459.803556	6483.552561	8.390067	-0.089364	4.344992
460.326024	6491.608036	8.395072	-0.089466	4.347644
460.905248	6499.616069	8.400077	-0.089579	4.350280
460.792475	6507.712016	8.405082	-0.089563	4.352938
461.257336	6515.699358	8.410086	-0.089655	4.355563
461.625941	6523.672858	8.415091	-0.089729	4.358182
461.815678	6531.657065	8.420096	-0.089769	4.360800
462.129899	6539.689253	8.425101	-0.089833	4.363434
463.117727	6547.633029	8.430106	-0.090022	4.366042
463.394399	6555.704695	8.435110	-0.090079	4.368685
463.333248	6563.767365	8.440115	-0.090073	4.371321
463.342586	6571.780882	8.445120	-0.090080	4.373940
463.645013	6579.829582	8.450125	-0.090141	4.376571
463.972373	6587.730636	8.455130	-0.090207	4.379152
464.415659	6595.834249	8.460134	-0.090295	4.381799
464.573897	6603.776163	8.465139	-0.090330	4.384389
464.467170	6611.911092	8.470144	-0.090315	4.387039
464.832191	6619.905585	8.475149	-0.090388	4.389645
465.194641	6627.930941	8.480154	-0.090461	4.392259
465.442231	6635.973013	8.485158	-0.090512	4.394876
465.528486	6644.001880	8.490163	-0.090533	4.397486
466.142327	6651.924814	8.495168	-0.090653	4.400064
466.549228	6659.974767	8.500173	-0.090734	4.402680
466.634671	6667.996065	8.505178	-0.090755	4.405283
467.161444	6676.064287	8.510182	-0.090858	4.407902
467.663277	6684.072445	8.515187	-0.090957	4.410500
467.979497	6692.102300	8.520192	-0.091021	4.413103
468.250270	6700.137820	8.525197	-0.091077	4.415705
468.170694	6708.180365	8.530202	-0.091067	4.418307
468.653038	6716.262500	8.535206	-0.091162	4.420922
468.383970	6724.207615	8.540211	-0.091117	4.423488
468.647950	6732.222847	8.545216	-0.091171	4.426078
469.448836	6740.178909	8.550221	-0.091326	4.428650
469.694202	6748.287401	8.555226	-0.091377	4.431266
470.138944	6756.274554	8.560231	-0.091465	4.433843
470.495847	6764.297982	8.565235	-0.091536	4.436430
470.839627	6772.268250	8.570240	-0.091605	4.438997
470.640554	6780.409858	8.575245	-0.091574	4.441616
471.143246	6788.277473	8.580250	-0.091672	4.444149
470.964854	6796.423359	8.585255	-0.091644	4.446766
471.245014	6804.336744	8.590259	-0.091702	4.449309
471.753925	6812.388587	8.595264	-0.091802	4.451896
471.949266	6820.388539	8.600269	-0.091843	4.454464
472.430568	6828.379371	8.605274	-0.091938	4.457028
472.607075	6836.430944	8.610279	-0.091976	4.459609
472.580494	6844.482278	8.615283	-0.091976	4.462188
472.654509	6852.445177	8.620288	-0.091995	4.464737
473.012380	6860.461551	8.625293	-0.092067	4.467303
473.120342	6868.486006	8.630298	-0.092092	4.469869
473.474791	6876.551966	8.635303	-0.092164	4.472447
473.332330	6884.596870	8.640307	-0.092142	4.475016
473.990597	6892.521690	8.645312	-0.092270	4.477548
474.038798	6900.569528	8.650317	-0.092284	4.480115
474.115991	6908.522712	8.655322	-0.092304	4.482651
474.622311	6916.521303	8.660327	-0.092403	4.485201
474.864408	6924.575864	8.665331	-0.092453	4.487767
475.360447	6932.607627	8.670336	-0.092551	4.490325
475.783520	6940.647963	8.675341	-0.092635	4.492883
475.738496	6948.654153	8.680346	-0.092632	4.495428
476.579584	6956.636323	8.685351	-0.092794	4.497967
476.798290	6964.622285	8.690355	-0.092839	4.500503
476.431348	6972.731331	8.695360	-0.092776	4.503075
476.768436	6980.727161	8.700365	-0.092844	4.505612
477.770122	6988.648834	8.705370	-0.093036	4.508126
477.625093	6996.813721	8.710375	-0.093014	4.510712
477.876814	7004.738611	8.715379	-0.093066	4.513222
477.669977	7012.792905	8.720384	-0.093033	4.515770
478.413958	7020.749748	8.725389	-0.093177	4.518288
478.466343	7028.799825	8.730394	-0.093192	4.520833
478.743941	7036.756502	8.735399	-0.093248	4.523347
479.257468	7044.776933	8.740403	-0.093349	4.525881
479.228739	7052.797925	8.745408	-0.093349	4.528411
479.819959	7060.896311	8.750413	-0.093464	4.530967
480.067193	7068.845839	8.755418	-0.093516	4.533473
480.496587	7076.921316	8.760423	-0.093601	4.536017
480.493996	7084.855169	8.765427	-0.093605	4.538515
480.486491	7092.965149	8.770432	-0.093609	4.541067
480.756624	7100.898821	8.775437	-0.093665	4.543562
480.995407	7108.972340	8.780442	-0.093714	4.546100
481.662001	7116.942991	8.785447	-0.093844	4.548605
481.858096	7125.027058	8.790451	-0.093885	4.551143
482.246557	7132.971080	8.795456	-0.093963	4.553636
482.284015	7141.049419	8.800461	-0.093975	4.556170
482.777080	7148.972900	8.805466	-0.094072	4.558654
482.522147	7157.130896	8.810471	-0.094030	4.561209
482.521006	7165.054417	8.815475	-0.094035	4.563689
483.145168	7173.037487	8.820480	-0.094156	4.566188
483.612918	7181.053033	8.825485	-0.094248	4.568695
483.564422	7189.122954	8.830490	-0.094245	4.571217
484.187687	7197.107805	8.835495	-0.094366	4.573712
484.192141	7205.169426	8.840499	-0.094372	4.576229
484.138740	7213.173721	8.845504	-0.094367	4.578726
484.964680	7221.157233	8.850509	-0.094526	4.581217
485.363896	7229.112262	8.855514	-0.094606	4.583697
485.525441	7237.247227	8.860519	-0.094641	4.586231
485.585003	7245.207619	8.865523	-0.094657	4.588709
485.564695	7253.308152	8.870528	-0.094659	4.591229
485.995647	7261.282930	8.875533	-0.094744	4.593710
486.115696	7269.267300	8.880538	-0.094772	4.596192
486.800973	7277.169726	8.885543	-0.094904	4.598647
487.267457	7285.262414	8.890547	-0.094996	4.601160
487.221843	7293.242445	8.895552	-0.094993	4.603636
487.145371	7301.401054	8.900557	-0.094984	4.606166
487.573193	7309.311982	8.905562	-0.095069	4.608618
487.901657	7317.376725	8.910567	-0.095135	4.611117
488.468286	7325.315359	8.915571	-0.095246	4.613575
488.617155	7333.359170	8.920576	-0.095279	4.616064
489.185623	7341.356176	8.925581	-0.095390	4.618538
489.054017	7349.443638	8.930586	-0.095371	4.621038
489.134344	7357.414862	8.935591	-0.095391	4.623500
489.096027	7365.495695	8.940595	-0.095389	4.625995
489.445444	7373.472239	8.945600	-0.095459	4.628457
489.418461	7381.533442	8.950605	-0.095459	4.630943
489.650007	7389.459034	8.955610	-0.095507	4.633387
489.962857	7397.523681	8.960615	-0.095571	4.635872
490.213584	7405.462990	8.965619	-0.095623	4.638316
490.708041	7413.482698	8.970624	-0.095720	4.640785
490.888050	7421.506806	8.975629	-0.095759	4.643253
491.285125	7429.504881	8.980634	-0.095838	4.645712
491.642926	7437.600832	8.985639	-0.095910	4.648199
492.262750	7445.595730	8.990643	-0.096030	4.650655
492.029618	7453.632899	8.995648	-0.095992	4.653122
492.342431	7461.648444	9.000653	-0.096056	4.655580
492.607060	7469.642826	9.005658	-0.096110	4.658032
492.907555	7477.689481	9.010663	-0.096171	4.660497
493.392373	7485.633799	9.015667	-0.096267	4.662930
493.808590	7493.656794	9.020672	-0.096349	4.665386
494.131118	7501.725830	9.025677	-0.096415	4.667855
494.747694	7509.690702	9.030682	-0.096535	4.670290
494.710980	7517.852427	9.035687	-0.096533	4.672784
495.261833	7525.807500	9.040691	-0.096641	4.675214
495.324589	7533.768547	9.045696	-0.096658	4.677644
495.651429	7541.803172	9.050701	-0.096724	4.680096
496.125538	7549.738199	9.055706	-0.096817	4.682515
496.097675	7557.796620	9.060711	-0.096817	4.684972
496.744442	7565.758277	9.065715	-0.096943	4.687396
496.583739	7573.895467	9.070720	-0.096918	4.689874
497.291585	7581.891729	9.075725	-0.097055	4.692307
497.209735	7589.865374	9.080730	-0.097045	4.694733
497.646111	7597.952302	9.085735	-0.097131	4.697190
497.811252	7605.883058	9.090739	-0.097167	4.699600
498.458126	7613.919049	9.095744	-0.097293	4.702040
498.584760	7621.938283	9.100749	-0.097322	4.704473
498.746380	7629.991764	9.105754	-0.097357	4.706916
499.264624	7637.996887	9.110759	-0.097459	4.709343
499.267403	7646.087893	9.115763	-0.097464	4.711795
499.352241	7654.042364	9.120768	-0.097485	4.714204
500.217963	7662.052139	9.125773	-0.097652	4.716627
499.926927	7670.001280	9.130778	-0.097603	4.719033
499.943678	7678.142239	9.135783	-0.097611	4.721495
500.505142	7686.029734	9.140787	-0.097721	4.723878
500.849230	7694.091523	9.145792	-0.097790	4.726313
501.311942	7702.064340	9.150797	-0.097881	4.728720
501.650731	7710.142941	9.155802	-0.097950	4.731157
502.037123	7718.169264	9.160807	-0.098027	4.733577
501.969652	7726.226401	9.165811	-0.098019	4.736006
502.450622	7734.132383	9.170816	-0.098114	4.738387
502.986099	7742.258647	9.175821	-0.098219	4.740834
503.226493	7750.201182	9.180826	-0.098269	4.743224
503.502238	7758.283058	9.185831	-0.098326	4.745655
503.762561	7766.295325	9.190835	-0.098379	4.748063
504.256064	7774.317993	9.195840	-0.098476	4.750473
504.491275	7782.304128	9.200845	-0.098525	4.752871
504.279793	7790.323542	9.205850	-0.098491	4.755280
504.761349	7798.376395	9.210855	-0.098586	4.757695
504.798138	7806.376141	9.215859	-0.098598	4.760094
505.215816	7814.296192	9.220864	-0.098681	4.762467
505.923062	7822.299353	9.225869	-0.098818	4.764863
505.969297	7830.414760	9.230874	-0.098832	4.767293
506.246580	7838.386508	9.235879	-0.098888	4.769678
506.432654	7846.459512	9.240883	-0.098928	4.772093
506.908457	7854.434341	9.245888	-0.099022	4.774476
506.594092	7862.521662	9.250893	-0.098969	4.776894
506.872122	7870.459664	9.255898	-0.099026	4.779264
507.196642	7878.543456	9.260903	-0.099091	4.781677
507.896528	7886.343849	9.265907	-0.099227	4.784002
507.980123	7894.519010	9.270912	-0.099248	4.786440
508.603125	7902.534102	9.275917	-0.099369	4.788827
508.550446	7910.556727	9.280922	-0.099364	4.791217
508.550660	7918.587147	9.285927	-0.099369	4.793609
508.602250	7926.609642	9.290931	-0.099384	4.795997
508.943052	7934.547490	9.295936	-0.099453	4.798357
509.207489	7942.701584	9.300941	-0.099507	4.800780
509.713053	7950.572033	9.305946	-0.099607	4.803118
510.328257	7958.599364	9.310951	-0.099726	4.805500
510.312669	7966.668640	9.315955	-0.099729	4.807895
510.560826	7974.623505	9.320960	-0.099780	4.810255
510.526377	7982.692139	9.325965	-0.099779	4.812648
510.889813	7990.121549	9.330970	-0.099851	4.814849
511.153332	7994.884989	9.335975	-0.099903	4.816260

511.476577	7997.494463	9.340979	-0.099965	4.817032
511.704669	7998.906772	9.345984	-0.100009	4.817449
511.857278	7999.429613	9.350989	-0.100037	4.817603
512.054423	8000.192378	9.355994	-0.100074	4.817828
512.562837	8000.212345	9.360999	-0.100169	4.817832
512.636337	8000.253455	9.366003	-0.100183	4.817844
512.360697	8000.270563	9.371008	-0.100131	4.817850
512.789409	8000.307303	9.376013	-0.100211	4.817859
513.144146	8000.236519	9.381018	-0.100277	4.817837
513.162309	8000.249427	9.386023	-0.100281	4.817841
513.104487	8000.280213	9.391027	-0.100270	4.817850
513.828474	8000.191561	9.396032	-0.100405	4.817821
514.042872	8000.156702	9.401037	-0.100444	4.817809
513.968649	8000.157738	9.406042	-0.100431	4.817810
513.952859	8000.215481	9.411047	-0.100428	4.817827
514.141705	8000.205552	9.416051	-0.100463	4.817823
513.998916	8000.200329	9.421056	-0.100436	4.817822
514.052768	8000.226400	9.426061	-0.100446	4.817830
514.251830	8000.201861	9.431066	-0.100483	4.817822
514.510974	8000.257244	9.436071	-0.100531	4.817837
514.790105	8000.215940	9.441075	-0.100583	4.817824
514.489245	8000.252709	9.446080	-0.100527	4.817836
514.591780	8000.321647	9.451085	-0.100546	4.817856
514.491314	8000.230598	9.456090	-0.100528	4.817829
514.440274	8000.284672	9.461095	-0.100518	4.817846
514.564773	8000.261166	9.466099	-0.100541	4.817838
514.941392	8000.195970	9.471104	-0.100611	4.817817
514.951186	8000.264624	9.476109	-0.100613	4.817837
514.917649	8000.243056	9.481114	-0.100607	4.817831
515.309993	8000.221305	9.486119	-0.100680	4.817823
514.902883	8000.270245	9.491123	-0.100604	4.817839
515.297434	8000.216902	9.496128	-0.100677	4.817822
515.666862	8000.245418	9.501133	-0.100746	4.817829
515.532475	8000.235044	9.506138	-0.100721	4.817826
515.776863	8000.239621	9.511143	-0.100767	4.817827
515.694972	8000.245816	9.516147	-0.100751	4.817829
515.736938	8000.209525	9.521152	-0.100759	4.817818
515.422567	8000.304074	9.526157	-0.100701	4.817847
515.609023	8000.228756	9.531162	-0.100735	4.817824
515.826949	8000.323606	9.536167	-0.100776	4.817851
515.574379	8000.291498	9.541171	-0.100729	4.817843
515.994681	8000.245907	9.546176	-0.100807	4.817827
515.916514	8000.340702	9.551181	-0.100792	4.817856
515.479481	8000.331232	9.556186	-0.100711	4.817855
515.894752	8000.330896	9.561191	-0.100788	4.817853
515.797043	8000.290481	9.566195	-0.100770	4.817842
515.960237	8000.319186	9.571200	-0.100800	4.817849
515.695714	8000.378614	9.576205	-0.100751	4.817868
515.862025	8000.325142	9.581210	-0.100782	4.817852
516.501518	8000.275336	9.586215	-0.100901	4.817834
516.175068	8000.243215	9.591219	-0.100840	4.817826
516.638954	8000.185604	9.596224	-0.100926	4.817807
516.814916	8000.264039	9.601229	-0.100959	4.817829
516.457349	8000.259930	9.606234	-0.100893	4.817830
516.672182	8000.235620	9.611239	-0.100933	4.817822
516.402045	8000.267560	9.616243	-0.100882	4.817832
516.528487	8000.272544	9.621248	-0.100906	4.817833
516.524913	8000.357875	9.626253	-0.100905	4.817858
516.407210	8000.341416	9.631258	-0.100883	4.817854
515.942218	8000.430629	9.636263	-0.100797	4.817882
515.994793	8000.387112	9.641267	-0.100806	4.817869
516.123995	8000.352079	9.646272	-0.100830	4.817858
516.629121	8000.338283	9.651277	-0.100924	4.817852
516.543284	8000.319121	9.656282	-0.100908	4.817847
516.841092	8000.330796	9.661287	-0.100964	4.817849
516.885607	8000.299812	9.666291	-0.100972	4.817840
517.037487	8000.237699	9.671296	-0.101000	4.817821
516.856344	8000.277247	9.676301	-0.100966	4.817833
516.954784	8000.183792	9.681306	-0.100985	4.817805
517.171880	8000.276526	9.686311	-0.101025	4.817832
517.079490	8000.333168	9.691315	-0.101008	4.817849
516.593680	8000.367264	9.696320	-0.100917	4.817861
516.652448	8000.380760	9.701325	-0.100928	4.817865
516.727202	8000.348103	9.706330	-0.100942	4.817855
516.989580	8000.362430	9.711335	-0.100991	4.817858
516.485958	8000.425785	9.716339	-0.100897	4.817879
516.716567	8000.370079	9.721344	-0.100940	4.817861
516.420297	8000.427994	9.726349	-0.100885	4.817880
516.571304	8000.420684	9.731354	-0.100913	4.817877
516.586093	8000.469386	9.736359	-0.100916	4.817891
516.602137	8000.398987	9.741363	-0.100919	4.817870
516.437180	8000.425065	9.746368	-0.100888	4.817879
516.797624	8000.415507	9.751373	-0.100955	4.817874
517.119176	8000.380089	9.756378	-0.101015	4.817862
516.714909	8000.410091	9.761383	-0.100940	4.817873
517.026736	8000.338691	9.766387	-0.100998	4.817851
517.491409	8000.310610	9.771392	-0.101084	4.817840
517.492376	8000.326434	9.776397	-0.101084	4.817845
517.194211	8000.356914	9.781402	-0.101029	4.817855
516.640407	8000.431140	9.786407	-0.100926	4.817880
517.034580	8000.395716	9.791411	-0.100999	4.817867
517.209200	8000.348689	9.796416	-0.101031	4.817853
517.120073	8000.401162	9.801421	-0.101015	4.817869
517.265608	8000.325252	9.806426	-0.101042	4.817846
516.916205	8000.414025	9.811431	-0.100977	4.817873
516.778912	8000.440503	9.816435	-0.100951	4.817882
516.914538	8000.456162	9.821440	-0.100976	4.817886
517.192274	8000.424328	9.826445	-0.101028	4.817875
517.206662	8000.392908	9.831450	-0.101031	4.817866
517.369860	8000.435321	9.836455	-0.101061	4.817878
517.340779	8000.383244	9.841459	-0.101056	4.817862
516.758358	8000.474977	9.846464	-0.100947	4.817892
517.039632	8000.420003	9.851469	-0.100999	4.817875
517.098904	8000.409260	9.856474	-0.101010	4.817871
517.205613	8000.423448	9.861479	-0.101030	4.817875
517.682019	8000.321746	9.866483	-0.101119	4.817843
516.938614	8000.434346	9.871488	-0.100981	4.817879
517.627557	8000.417938	9.876493	-0.101109	4.817872
517.203549	8000.444491	9.881498	-0.101030	4.817881
517.342618	8000.449659	9.886503	-0.101056	4.817882
518.010733	8000.335967	9.891507	-0.101180	4.817846
517.715340	8000.338024	9.896512	-0.101125	4.817847
517.579273	8000.418281	9.901517	-0.101100	4.817872
517.972125	8000.296397	9.906522	-0.101173	4.817834
517.804676	8000.345631	9.911527	-0.101141	4.817849
517.680676	8000.361758	9.916531	-0.101118	4.817855
517.984283	8000.348220	9.921536	-0.101175	4.817849
518.218244	8000.323133	9.926541	-0.101218	4.817841
517.982077	8000.290203	9.931546	-0.101174	4.817832
518.038509	8000.372187	9.936551	-0.101185	4.817856
518.297893	8000.359064	9.941555	-0.101233	4.817851
517.932767	8000.373817	9.946560	-0.101165	4.817857
518.223105	8000.379062	9.951565	-0.101219	4.817857
518.000397	8000.363192	9.956570	-0.101178	4.817854
517.721955	8000.417148	9.961575	-0.101126	4.817871
518.043024	8000.384886	9.966579	-0.101186	4.817860
518.012525	8000.408689	9.971584	-0.101180	4.817867
518.180560	8000.401626	9.976589	-0.101211	4.817864
517.683439	8000.418689	9.981594	-0.101118	4.817872
518.159235	8000.311707	9.986599	-0.101207	4.817838
517.835114	8000.437741	9.991603	-0.101147	4.817876
517.693774	8000.437806	9.996608	-0.101120	4.817877
518.368233	8000.427516	10.001613	-0.101246	4.817871
518.390442	8000.362475	10.006618	-0.101250	4.817852
518.296242	8000.382195	10.011623	-0.101232	4.817858
517.934360	8000.428620	10.016627	-0.101165	4.817873
517.840573	8000.465213	10.021632	-0.101147	4.817885
518.442662	8000.458096	10.026637	-0.101260	4.817880
517.856752	8000.408516	10.031642	-0.101150	4.817868
518.251695	8000.422652	10.036647	-0.101224	4.817870
518.308239	8000.412924	10.041651	-0.101234	4.817867
518.176790	8000.401535	10.046656	-0.101210	4.817864
517.769725	8000.452578	10.051661	-0.101134	4.817881
517.787708	8000.457052	10.056666	-0.101137	4.817882
517.699497	8000.412554	10.061671	-0.101121	4.817870
518.005467	8000.412754	10.066675	-0.101178	4.817868
518.530767	8000.383443	10.071680	-0.101276	4.817857
518.228020	8000.450751	10.076685	-0.101219	4.817879
518.048146	8000.412308	10.081690	-0.101186	4.817868
517.993864	8000.374625	10.086695	-0.101176	4.817857
518.634508	8000.384931	10.091699	-0.101295	4.817857
518.840977	8000.295143	10.096704	-0.101333	4.817830
518.673183	8000.383376	10.101709	-0.101302	4.817857
518.868524	8000.329270	10.106714	-0.101338	4.817840
519.061518	8000.346814	10.111719	-0.101374	4.817844
518.582719	8000.398929	10.116723	-0.101285	4.817862
518.705959	8000.360647	10.121728	-0.101308	4.817850
518.669702	8000.427589	10.126733	-0.101301	4.817870
518.905711	8000.356149	10.131738	-0.101345	4.817848
518.950284	8000.368386	10.136743	-0.101353	4.817851
518.964707	8000.356996	10.141747	-0.101356	4.817848
519.290052	8000.300551	10.146752	-0.101416	4.817830
518.518670	8000.427502	10.151757	-0.101273	4.817871
518.421244	8000.366003	10.156762	-0.101255	4.817853
518.666316	8000.429630	10.161767	-0.101300	4.817871
518.659378	8000.428473	10.166771	-0.101299	4.817870
518.352042	8000.414542	10.171776	-0.101242	4.817867
519.030667	8000.396936	10.176781	-0.101368	4.817859
518.633831	8000.399633	10.181786	-0.101294	4.817862
518.477287	8000.417398	10.186791	-0.101265	4.817868
518.517496	8000.419030	10.191795	-0.101272	4.817868
518.734643	8000.347317	10.196800	-0.101313	4.817846
518.385150	8000.446630	10.201805	-0.101248	4.817877
518.233873	8000.426521	10.206810	-0.101219	4.817872
518.610249	8000.416143	10.211815	-0.101289	4.817867
519.176637	8000.309417	10.216819	-0.101395	4.817833
519.145987	8000.241502	10.221824	-0.101389	4.817813
519.226461	8000.325944	10.226829	-0.101404	4.817837
518.705625	8000.412240	10.231834	-0.101307	4.817865
518.748633	8000.407587	10.236839	-0.101315	4.817864
518.587697	8000.467457	10.241843	-0.101285	4.817882
518.917271	8000.340442	10.246848	-0.101346	4.817843
518.868758	8000.406153	10.251853	-0.101337	4.817863
518.775836	8000.390048	10.256858	-0.101320	4.817858
518.660381	8000.434762	10.261863	-0.101298	4.817872
518.926837	8000.406984	10.266867	-0.101348	4.817863
518.615795	8000.448872	10.271872	-0.101290	4.817876
518.732772	8000.373603	10.276877	-0.101312	4.817854
518.345926	8000.456563	10.281882	-0.101240	4.817880
518.738319	8000.450634	10.286887	-0.101313	4.817876
518.560519	8000.358456	10.291891	-0.101280	4.817850
518.485272	8000.472273	10.296896	-0.101266	4.817884
518.852537	8000.415380	10.301901	-0.101334	4.817866
519.023384	8000.383057	10.306906	-0.101366	4.817855
519.027570	8000.407362	10.311911	-0.101366	4.817862
518.900857	8000.435046	10.316915	-0.101343	4.817871
518.344735	8000.422790	10.321920	-0.101239	4.817870
518.838698	8000.499503	10.326925	-0.101331	4.817891
519.006479	8000.415480	10.331930	-0.101362	4.817865
519.223314	8000.388039	10.336935	-0.101403	4.817856
519.715399	8000.327679	10.341939	-0.101494	4.817836
519.670178	8000.305938	10.346944	-0.101486	4.817830
519.273169	8000.433028	10.351949	-0.101412	4.817869
519.112797	8000.391702	10.356954	-0.101382	4.817857
519.372774	8000.433409	10.361959	-0.101430	4.817869
518.926548	8000.460691	10.366963	-0.101347	4.817879
519.113867	8000.438095	10.371968	-0.101382	4.817871
519.358677	8000.426872	10.376973	-0.101428	4.817867
519.202477	8000.376118	10.381978	-0.101399	4.817852
518.694349	8000.454162	10.386983	-0.101304	4.817878
518.859732	8000.471309	10.391987	-0.101335	4.817882
518.882741	8000.476910	10.396992	-0.101339	4.817884
519.169132	8000.367191	10.401997	-0.101392	4.817850
518.850431	8000.441649	10.407002	-0.101333	4.817873
518.833538	8000.440348	10.412007	-0.101330	4.817873
519.022780	8000.482086	10.417011	-0.101365	4.817885
518.841905	8000.490011	10.422016	-0.101331	4.817888
519.331024	8000.393765	10.427021	-0.101422	4.817857
519.305596	8000.420804	10.432026	-0.101417	4.817865
519.604894	8000.440941	10.437031	-0.101473	4.817870
519.258964	8000.465456	10.442035	-0.101409	4.817879
519.328267	8000.463293	10.447040	-0.101422	4.817878
519.317980	8000.475792	10.452045	-0.101420	4.817881
518.984334	8000.463587	10.457050	-0.101357	4.817879
519.246900	8000.469488	10.462055	-0.101406	4.817880
519.394033	8000.386221	10.467059	-0.101434	4.817855
518.828576	8000.481358	10.472064	-0.101328	4.817885
518.845906	8000.462630	10.477069	-0.101332	4.817880
519.233388	8000.422897	10.482074	-0.101404	4.817866
519.452998	8000.426068	10.487079	-0.101445	4.817866
518.891744	8000.458014	10.492083	-0.101340	4.817878
519.346756	8000.465642	10.497088	-0.101425	4.817878
519.558743	8000.476083	10.502093	-0.101464	4.817881
518.788398	8000.396423	10.507098	-0.101321	4.817860
518.995890	8000.253939	10.512103	-0.101359	4.817817
519.113118	8000.406381	10.517107	-0.101381	4.817862
518.722952	8000.270020	10.522112	-0.101308	4.817823
519.043285	8000.343168	10.527117	-0.101368	4.817843
519.458492	8000.480943	10.532122	-0.101445	4.817882
519.294185	8000.411096	10.537127	-0.101415	4.817862
519.102759	8000.379863	10.542131	-0.101379	4.817854
519.067961	8000.509025	10.547136	-0.101372	4.817892
519.578540	8000.434174	10.552141	-0.101467	4.817868
519.858507	8000.423459	10.557146	-0.101520	4.817864
520.048789	8000.467323	10.562151	-0.101555	4.817876
519.387030	8000.292241	10.567155	-0.101432	4.817827
519.218279	8000.264499	10.572160	-0.101400	4.817819
519.459511	8000.392380	10.577165	-0.101445	4.817856
520.019778	8000.373066	10.582170	-0.101549	4.817848
520.141099	8000.419096	10.587175	-0.101572	4.817861
520.066964	8000.394828	10.592179	-0.101558	4.817854
520.109549	8000.391224	10.597184	-0.101566	4.817853
519.984757	8000.453725	10.602189	-0.101543	4.817872
519.739403	8000.425928	10.607194	-0.101497	4.817865
520.211374	8000.393743	10.612199	-0.101585	4.817853
520.356712	8000.344184	10.617203	-0.101612	4.817838
519.846068	8000.392673	10.622208	-0.101517	4.817855
519.725480	8000.466831	10.627213	-0.101494	4.817877
519.321434	8000.493668	10.632218	-0.101419	4.817887
519.637223	8000.472929	10.637223	-0.101478	4.817879
519.443538	8000.413199	10.642227	-0.101442	4.817862
519.553759	8000.456958	10.647232	-0.101462	4.817875
519.857342	8000.480321	10.652237	-0.101519	4.817881
519.319866	8000.485198	10.657242	-0.101419	4.817884
519.580892	8000.377222	10.662247	-0.101467	4.817851
519.580283	8000.468927	10.667251	-0.101467	4.817878
519.607750	8000.488298	10.672256	-0.101472	4.817884
519.840368	8000.487442	10.677261	-0.101515	4.817883
519.962162	8000.413295	10.682266	-0.101538	4.817860
520.130235	8000.439970	10.687271	-0.101569	4.817867
520.325320	8000.414324	10.692275	-0.101606	4.817859
519.972731	8000.410277	10.697280	-0.101540	4.817859
519.940358	8000.400319	10.702285	-0.101534	4.817857
519.978423	8000.415626	10.707290	-0.101541	4.817861
519.341598	8000.497080	10.712295	-0.101422	4.817888
519.649284	8000.470953	10.717299	-0.101480	4.817879
519.488157	8000.390608	10.722304	-0.101449	4.817856
519.845247	8000.501191	10.727309	-0.101516	4.817887
520.239442	8000.384597	10.732314	-0.101589	4.817851
520.287247	8000.431672	10.737319	-0.101598	4.817864
519.603565	8000.277356	10.742323	-0.101471	4.817822
519.990879	8000.330392	10.747328	-0.101543	4.817836
520.328302	8000.445962	10.752333	-0.101606	4.817868
519.980804	8000.454640	10.757338	-0.101541	4.817872
519.591216	8000.512258	10.762343	-0.101468	4.817891
520.106125	8000.427982	10.767347	-0.101564	4.817864
520.681226	8000.317167	10.772352	-0.101671	4.817829
520.299411	8000.354867	10.777357	-0.101600	4.817842
520.261676	8000.424953	10.782362	-0.101593	4.817862
519.803742	8000.503721	10.787367	-0.101508	4.817888
519.970196	8000.469227	10.792371	-0.101539	4.817877
519.911410	8000.400904	10.797376	-0.101528	4.817857
520.011588	8000.484580	10.802381	-0.101546	4.817881
519.941581	8000.448775	10.807386	-0.101533	4.817871
520.205078	8000.443094	10.812391	-0.101582	4.817868
520.059266	8000.388272	10.817395	-0.101555	4.817852
520.348157	8000.417748	10.822400	-0.101609	4.817860
520.287804	8000.437957	10.827405	-0.101598	4.817866
519.777014	8000.408430	10.832410	-0.101502	4.817860
519.876616	8000.492098	10.837415	-0.101521	4.817884
520.159021	8000.443467	10.842419	-0.101574	4.817868
519.599358	8000.484921	10.847424	-0.101469	4.817883
519.767986	8000.293379	10.852429	-0.101501	4.817826
519.881936	8000.454212	10.857434	-0.101522	4.817873
520.073579	8000.468577	10.862439	-0.101558	4.817876
520.135952	8000.485289	10.867443	-0.101569	4.817881
519.770815	8000.488441	10.872448	-0.101501	4.817883
520.222408	8000.454907	10.877453	-0.101585	4.817872
519.829102	8000.392289	10.882458	-0.101512	4.817855
520.386061	8000.375038	10.887463	-0.101615	4.817847
519.890363	8000.479616	10.892467	-0.101523	4.817880
519.836128	8000.413467	10.897472	-0.101513	4.817861
520.314165	8000.369773	10.902477	-0.101602	4.817846
520.611547	8000.383559	10.907482	-0.101657	4.817849
520.773873	8000.345843	10.912487	-0.101688	4.817837
520.779642	8000.381768	10.917491	-0.101689	4.817847
520.582598	8000.413706	10.922496	-0.101652	4.817858
520.918484	8000.414344	10.927501	-0.101714	4.817857
520.355055	8000.424115	10.932506	-0.101609	4.817862
520.608850	8000.465735	10.937511	-0.101657	4.817873
521.262300	8000.380302	10.942515	-0.101778	4.817845
520.899298	8000.342367	10.947520	-0.101711	4.817835
520.903629	8000.369837	10.952525	-0.101711	4.817843
520.610723	8000.409877	10.957530	-0.101657	4.817857
520.912270	8000.356252	10.962535	-0.101713	4.817839
520.430051	8000.427289	10.967539	-0.101623	4.817862
520.360007	8000.402026	10.972544	-0.101610	4.817855
520.909586	8000.397321	10.977549	-0.101712	4.817852
520.003622	8000.456959	10.982554	-0.101544	4.817873
519.718957	8000.418051	10.987559	-0.101491	4.817863
520.029970	8000.399352	10.992563	-0.101548	4.817856
519.882448	8000.474175	10.997568	-0.101521	4.817879
520.366069	8000.451647	11.002573	-0.101611	4.817870
520.154085	8000.470718	11.007578	-0.101572	4.817876
520.074678	8000.395771	11.012583	-0.101557	4.817855
520.297997	8000.342068	11.017587	-0.101598	4.817838
520.349071	8000.428197	11.022592	-0.101608	4.817863
520.326749	8000.465825	11.027597	-0.101604	4.817874
519.822247	8000.376297	11.032602	-0.101510	4.817850
519.928927	8000.263981	11.037607	-0.101529	4.817816
520.106230	8000.513231	11.042611	-0.101562	4.817889
519.747984	8000.403680	11.047616	-0.101496	4.817858
519.806939	8000.259047	11.052621	-0.101506	4.817815
519.875183	8000.484580	11.057626	-0.101519	4.817882
519.766622	8000.400779	11.062631	-0.101499	4.817857
519.982365	8000.385973	11.067635	-0.101539	4.817852
519.755712	8000.299410	11.072640	-0.101497	4.817827
519.988555	8000.294340	11.077645	-0.101540	4.817825
520.482057	8000.442740	11.082650	-0.101632	4.817867
520.082822	8000.277775	11.087655	-0.101558	4.817820
520.246877	8000.165234	11.092659	-0.101588	4.817786
520.272273	8000.312135	11.097664	-0.101593	4.817829
520.219152	8000.361968	11.102669	-0.101583	4.817844
520.145184	8000.439963	11.107674	-0.101569	4.817867
519.841666	8000.293252	11.112679	-0.101513	4.817825
520.344310	8000.494495	11.117683	-0.101606	4.817883
520.093560	8000.496138	11.122688	-0.101559	4.817884
520.189010	8000.403688	11.127693	-0.101577	4.817857
520.125790	8000.419639	11.132698	-0.101565	4.817862
519.948184	8000.526709	11.137703	-0.101532	4.817894
520.169540	8000.420266	11.142707	-0.101573	4.817862
519.822200	8000.473224	11.147712	-0.101509	4.817879
520.194105	8000.497576	11.152717	-0.101578	4.817884
520.749830	8000.428650	11.157722	-0.101681	4.817862
520.458873	8000.465555	11.162727	-0.101627	4.817874
520.558545	8000.454343	11.167731	-0.101646	4.817870
520.589800	8000.409460	11.172736	-0.101651	4.817857
520.536282	8000.392870	11.177741	-0.101641	4.817852
520.595557	8000.426406	11.182746	-0.101653	4.817862
520.485227	8000.443784	11.187751	-0.101632	4.817867
520.919066	8000.393127	11.192755	-0.101713	4.817850
520.604112	8000.414925	11.197760	-0.101654	4.817858
521.022074	8000.409371	11.202765	-0.101732	4.817855
520.686185	8000.439300	11.207770	-0.101669	4.817865
520.657190	8000.452583	11.212775	-0.101664	4.817869
520.692515	8000.457309	11.217779	-0.101670	4.817870
520.745410	8000.457017	11.222784	-0.101680	4.817870
520.625877	8000.454231	11.227789	-0.101658	4.817870
520.381796	8000.436993	11.232794	-0.101612	4.817866
520.691063	8000.378208	11.237799	-0.101670	4.817847
520.931102	8000.442824	11.242803	-0.101715	4.817865
520.419146	8000.447013	11.247808	-0.101619	4.817868
520.476840	8000.467876	11.252813	-0.101630	4.817874
520.481717	8000.474269	11.257818	-0.101631	4.817876
520.719865	8000.360689	11.262823	-0.101675	4.817842
520.518768	8000.487451	11.267827	-0.101638	4.817880
520.249270	8000.501473	11.272832	-0.101587	4.817885
520.721678	8000.449265	11.277837	-0.101675	4.817868
520.703171	8000.444777	11.282842	-0.101672	4.817867
520.356487	8000.430272	11.287847	-0.101607	4.817864
520.694634	8000.503686	11.292851	-0.101670	4.817884
520.589555	8000.353515	11.297856	-0.101651	4.817840
520.161565	8000.529707	11.302861	-0.101571	4.817894
520.236565	8000.486511	11.307866	-0.101585	4.817881
520.415894	8000.411088	11.312871	-0.101618	4.817858
520.768227	8000.443591	11.317875	-0.101684	4.817866
520.648810	8000.437644	11.322880	-0.101661	4.817865
520.646078	8000.432331	11.327885	-0.101661	4.817863
520.757679	8000.470841	11.332890	-0.101682	4.817874
520.396798	8000.485649	11.337895	-0.101614	4.817880
520.775849	8000.474261	11.342899	-0.101685	4.817875
520.216228	8000.369175	11.347904	-0.101581	4.817846
520.097199	8000.282059	11.352909	-0.101558	4.817821
520.446503	8000.506388	11.357914	-0.101624	4.817886
520.620038	8000.409796	11.362919	-0.101656	4.817857
520.064403	8000.393325	11.367923	-0.101552	4.817854
520.109500	8000.390812	11.372928	-0.101561	4.817853
520.837616	8000.409773	11.377933	-0.101696	4.817856
520.549153	8000.318096	11.382938	-0.101642	4.817830
520.353524	8000.514516	11.387943	-0.101606	4.817889
520.253934	8000.292738	11.392947	-0.101587	4.817823
520.414990	8000.288738	11.397952	-0.101617	4.817822
520.158536	8000.437891	11.402957	-0.101570	4.817867
520.491667	8000.402645	11.407962	-0.101632	4.817855
520.879609	8000.440935	11.412967	-0.101704	4.817865
520.631009	8000.472126	11.417971	-0.101658	4.817875
520.378560	8000.480069	11.422976	-0.101610	4.817878
521.034698	8000.480069	11.427981	-0.101733	4.817876
520.463171	8000.512915	11.432986	-0.101626	4.817888
520.318785	8000.380098	11.437991	-0.101599	4.817849
520.344523	8000.399444	11.442995	-0.101604	4.817855
520.841398	8000.392922	11.448000	-0.101696	4.817851
520.369679	8000.158384	11.453005	-0.101608	4.817783
520.649981	8000.486085	11.458010	-0.101661	4.817879
520.499715	8000.476529	11.463015	-0.101633	4.817877
520.409836	8000.459413	11.468019	-0.101616	4.817872
519.919182	8000.470237	11.473024	-0.101525	4.817877
520.534126	8000.293581	11.478029	-0.101639	4.817822
520.473402	8000.464541	11.483034	-0.101628	4.817873
520.431850	8000.457612	11.488039	-0.101620	4.817872
520.313255	8000.501227	11.493043	-0.101598	4.817885
520.401941	8000.380215	11.498048	-0.101614	4.817849
520.048580	8000.207481	11.503053	-0.101548	4.817799
520.125850	8000.503780	11.508058	-0.101563	4.817886
520.432845	8000.435474	11.513063	-0.101620	4.817865
520.444899	8000.502063	11.518067	-0.101622	4.817885
520.036027	8000.395995	11.523072	-0.101546	4.817855
520.315929	8000.433775	11.528077	-0.101598	4.817865
520.568456	8000.493300	11.533082	-0.101645	4.817881
520.254913	8000.381230	11.538087	-0.101587	4.817850
520.379138	8000.346126	11.543091	-0.101610	4.817839
520.644001	8000.354170	11.548096	-0.101659	4.817840
520.249104	8000.267281	11.553101	-0.101585	4.817816
520.140438	8000.318419	11.558106	-0.101565	4.817832
520.497861	8000.228703	11.563111	-0.101632	4.817803
520.772441	8000.469876	11.568115	-0.101683	4.817874
520.270783	8000.390929	11.573120	-0.101589	4.817852
520.535365	8000.449573	11.578125	-0.101639	4.817869
520.758716	8000.506568	11.583130	-0.101680	4.817885
520.635607	8000.477374	11.588135	-0.101657	4.817876
520.171249	8000.280894	11.593139	-0.101571	4.817820
520.039055	8000.437114	11.598144	-0.101546	4.817867
520.190019	8000.307516	11.603149	-0.101574	4.817828
520.199691	8000.261267	11.608154	-0.101576	4.817814
521.115345	8000.456890	11.613159	-0.101746	4.817868
520.903693	8000.395841	11.618163	-0.101707	4.817851
520.549428	8000.406529	11.623168	-0.101641	4.817856
520.313099	8000.210184	11.628173	-0.101597	4.817799
520.371235	8000.524130	11.633178	-0.101608	4.817891
519.980662	8000.099953	11.638183	-0.101535	4.817768
520.692098	8000.333730	11.643187	-0.101667	4.817834
520.826334	8000.462179	11.648192	-0.101692	4.817871
521.115037	8000.395717	11.653197	-0.101746	4.817850
521.036411	8000.516871	11.658202	-0.101731	4.817886
521.045688	8000.358864	11.663207	-0.101733	4.817840
520.847658	8000.507809	11.668211	-0.101696	4.817885
520.760054	8000.484400	11.673216	-0.101680	4.817878
520.801446	8000.417524	11.678221	-0.101687	4.817858
520.856422	8000.481572	11.683226	-0.101698	4.817877
520.843528	8000.460298	11.688231	-0.101695	4.817871
521.050770	8000.404254	11.693235	-0.101734	4.817853
520.680104	8000.295575	11.698240	-0.101665	4.817822
520.703704	8000.311727	11.703245	-0.101669	4.817827
520.651233	8000.475428	11.708250	-0.101659	4.817876
520.466668	8000.339921	11.713255	-0.101625	4.817837
520.891442	8000.424076	11.718259	-0.101704	4.817860
520.378008	8000.521018	11.723264	-0.101608	4.817891
520.734365	8000.421799	11.728269	-0.101675	4.817860
520.697873	8000.510879	11.733274	-0.101668	4.817886
521.211373	8000.455050	11.738279	-0.101763	4.817867
520.460651	8000.397801	11.743283	-0.101624	4.817854
520.284438	8000.316183	11.748288	-0.101591	4.817830
520.551543	8000.013262	11.753293	-0.101640	4.817739
520.918131	8000.508781	11.758298	-0.101709	4.817885
520.781686	8000.278033	11.763303	-0.101683	4.817817
521.102048	8000.492460	11.768307	-0.101743	4.817879
520.983131	8000.448567	11.773312	-0.101721	4.817867
521.146505	8000.485718	11.778317	-0.101751	4.817877
521.206301	8000.474983	11.783322	-0.101762	4.817873
520.906081	8000.418979	11.788327	-0.101706	4.817858
520.969995	8000.429389	11.793331	-0.101718	4.817861
520.998107	8000.488832	11.798336	-0.101723	4.817878
521.120414	8000.417855	11.803341	-0.101746	4.817857
520.873957	8000.510224	11.808346	-0.101700	4.817885
520.782424	8000.486758	11.813351	-0.101683	4.817879
521.209276	8000.381179	11.818355	-0.101762	4.817846
521.077122	8000.496287	11.823360	-0.101738	4.817880
521.246874	8000.402802	11.828365	-0.101769	4.817852
521.488899	8000.438984	11.833370	-0.101814	4.817862
521.411582	8000.455785	11.838375	-0.101800	4.817867
521.542287	8000.470325	11.843379	-0.101824	4.817871
521.280063	8000.486559	11.848384	-0.101775	4.817876
521.525874	8000.489059	11.853389	-0.101821	4.817876
521.495973	8000.431693	11.858394	-0.101816	4.817859
521.617553	8000.343836	11.863399	-0.101838	4.817833
520.868997	8000.281348	11.868403	-0.101699	4.817817
521.146948	8000.457209	11.873408	-0.101750	4.817868
520.784835	8000.225305	11.878413	-0.101683	4.817801
521.242003	8000.455416	11.883418	-0.101768	4.817867
521.052340	8000.519088	11.888423	-0.101733	4.817887
520.986872	8000.413766	11.893427	-0.101721	4.817856
520.929082	8000.495160	11.898432	-0.101710	4.817881
521.658790	8000.463544	11.903437	-0.101846	4.817868
521.396233	8000.470285	11.908442	-0.101797	4.817871
520.733815	8000.438560	11.913447	-0.101673	4.817865
520.595908	8000.236258	11.918451	-0.101647	4.817805
520.976567	8000.498996	11.923456	-0.101718	4.817881
520.827641	7999.971828	11.928461	-0.101690	4.817726
521.082071	8000.505789	11.933466	-0.101738	4.817883
521.181686	8000.406018	11.938471	-0.101756	4.817853
521.307762	8000.515374	11.943475	-0.101780	4.817885
521.063928	8000.427503	11.948480	-0.101734	4.817860
521.296705	8000.396077	11.953485	-0.101778	4.817850
521.170768	8000.441694	11.958490	-0.101754	4.817864
521.020777	8000.473258	11.963495	-0.101726	4.817874
521.348978	8000.499089	11.968499	-0.101787	4.817880
521.022784	8000.408972	11.973504	-0.101727	4.817855
520.609436	8000.398774	11.978509	-0.101650	4.817853
521.001817	8000.441345	11.983514	-0.101723	4.817864
520.640125	8000.418189	11.988519	-0.101655	4.817859
520.981836	8000.356711	11.993523	-0.101719	4.817839
521.177118	8000.469176	11.998528	-0.101755	4.817872
521.327843	8000.377524	12.003533	-0.101783	4.817844
521.465627	8000.495484	12.008538	-0.101809	4.817878
521.462643	8000.472245	12.013543	-0.101808	4.817872
520.741788	8000.160300	12.018547	-0.101674	4.817782
520.636827	8000.290560	12.023552	-0.101654	4.817821
521.221536	8000.428686	12.028557	-0.101763	4.817860
521.037670	8000.497713	12.033562	-0.101729	4.817881
521.058205	8000.416830	12.038567	-0.101733	4.817857
520.595958	8000.320531	12.043571	-0.101647	4.817830
520.826566	8000.235307	12.048576	-0.101689	4.817804
521.278792	8000.500137	12.053581	-0.101774	4.817881
521.035756	8000.363782	12.058586	-0.101728	4.817841
520.918230	8000.386327	12.063591	-0.101707	4.817848
520.982324	8000.255470	12.068595	-0.101718	4.817809
521.003016	8000.174590	12.073600	-0.101722	4.817785
521.336241	8000.246878	12.078605	-0.101784	4.817805
521.304256	8000.485730	12.083610	-0.101778	4.817876
521.114777	8000.407079	12.088615	-0.101743	4.817854
521.061089	8000.349370	12.093619	-0.101733	4.817837
520.900790	8000.511512	12.098624	-0.101703	4.817886
521.105544	8000.238257	12.103629	-0.101741	4.817804
521.278430	8000.491668	12.108634	-0.101773	4.817878
521.034629	8000.394310	12.113639	-0.101728	4.817850
521.029971	8000.490177	12.118643	-0.101727	4.817879
521.261263	8000.464001	12.123648	-0.101770	4.817870
521.273294	8000.222748	12.128653	-0.101772	4.817798
520.855766	8000.508734	12.133658	-0.101695	4.817885
521.214611	8000.387411	12.138663	-0.101761	4.817847
521.203349	8000.364052	12.143667	-0.101759	4.817841
520.895023	8000.468178	12.148672	-0.101702	4.817873
521.133252	8000.406258	12.153677	-0.101746	4.817853
520.873720	8000.521632	12.158682	-0.101698	4.817889
520.624449	8000.085786	12.163687	-0.101651	4.817761
520.949667	8000.395160	12.168691	-0.101712	4.817851
520.951205	8000.322436	12.173696	-0.101712	4.817829
521.249707	8000.510192	12.178701	-0.101768	4.817884
521.060728	8000.408355	12.183706	-0.101732	4.817854
521.305608	8000.422438	12.188711	-0.101778	4.817857
521.217703	8000.440140	12.193715	-0.101761	4.817863
520.920662	8000.433732	12.198720	-0.101706	4.817862
521.043735	8000.188815	12.203725	-0.101729	4.817789
521.362983	8000.482296	12.208730	-0.101788	4.817875
520.757348	8000.290093	12.213735	-0.101676	4.817821
520.704801	8000.011014	12.218739	-0.101666	4.817738
521.254017	8000.289891	12.223744	-0.101768	4.817818
520.980241	8000.402950	12.228749	-0.101717	4.817853
520.264457	7999.869704	12.233754	-0.101583	4.817698
520.527036	8000.066416	12.238759	-0.101632	4.817755
521.168577	7999.985023	12.243763	-0.101752	4.817729
520.933943	8000.517184	12.248768	-0.101708	4.817887
520.965587	8000.106483	12.253773	-0.101714	4.817765
521.146067	8000.136500	12.258778	-0.101747	4.817773
521.376524	8000.244200	12.263783	-0.101790	4.817804
520.981119	7999.958053	12.268787	-0.101717	4.817721
521.243087	8000.299194	12.273792	-0.101766	4.817821
521.106283	8000.530204	12.278797	-0.101740	4.817890
520.930966	8000.237746	12.283802	-0.101707	4.817804
520.942390	8000.349658	12.288807	-0.101709	4.817837
520.984313	7999.906429	12.293811	-0.101717	4.817706
520.950261	8000.421456	12.298816	-0.101711	4.817859
521.346161	8000.356545	12.303821	-0.101785	4.817838
520.814770	8000.194937	12.308826	-0.101685	4.817792
520.997942	8000.084780	12.313831	-0.101719	4.817759
521.103524	8000.241277	12.318835	-0.101739	4.817805
521.106119	8000.121128	12.323840	-0.101740	4.817769
520.897190	7999.880904	12.328845	-0.101700	4.817699
521.047923	8000.311099	12.333850	-0.101729	4.817826
520.899852	8000.048559	12.338855	-0.101701	4.817748
520.847634	7999.900210	12.343859	-0.101691	4.817705
520.867983	8000.006978	12.348864	-0.101695	4.817736
521.164797	8000.197866	12.353869	-0.101750	4.817792
521.509108	8000.411586	12.358874	-0.101815	4.817853
521.003908	8000.296742	12.363879	-0.101720	4.817822
521.237551	8000.137764	12.368883	-0.101764	4.817773
521.348134	8000.317529	12.373888	-0.101784	4.817826
521.495316	7999.935909	12.378893	-0.101812	4.817713
521.488975	8000.422878	12.383898	-0.101811	4.817857
521.373261	8000.077515	12.388903	-0.101789	4.817755
521.285921	7999.798987	12.393907	-0.101772	4.817673
521.592982	8000.505554	12.398912	-0.101830	4.817881
521.636911	8000.207830	12.403917	-0.101838	4.817793
521.755546	8000.437265	12.408922	-0.101860	4.817860
521.694155	8000.275071	12.413927	-0.101849	4.817812
521.648172	8000.276512	12.418931	-0.101840	4.817813
521.808325	8000.485463	12.423936	-0.101870	4.817874
522.303066	8000.414604	12.428941	-0.101962	4.817851
522.354016	8000.416393	12.433946	-0.101971	4.817851
521.912303	8000.456386	12.438951	-0.101889	4.817865
522.035200	8000.366440	12.443955	-0.101912	4.817838
522.140894	8000.445983	12.448960	-0.101932	4.817861
522.231049	8000.429363	12.453965	-0.101948	4.817856
522.555179	8000.390826	12.458970	-0.102009	4.817843
522.627406	8000.361294	12.463975	-0.102022	4.817834
522.823725	8000.402088	12.468979	-0.102059	4.817845
522.345664	8000.407817	12.473984	-0.101970	4.817849
522.541121	8000.425403	12.478989	-0.102006	4.817853
522.347727	8000.417330	12.483994	-0.101970	4.817852
522.415040	8000.369804	12.488999	-0.101982	4.817837
522.488627	8000.430961	12.494003	-0.101996	4.817855
522.525790	8000.374565	12.499008	-0.102003	4.817838
522.672392	8000.368250	12.504013	-0.102030	4.817836
522.838313	8000.381192	12.509018	-0.102061	4.817839
523.102658	8000.342844	12.514023	-0.102110	4.817826
523.007884	8000.331981	12.519027	-0.102092	4.817823
522.905314	8000.377937	12.524032	-0.102073	4.817837
522.963685	8000.445200	12.529037	-0.102084	4.817857
522.395166	8000.456999	12.534042	-0.101978	4.817863
522.264649	8000.448781	12.539047	-0.101954	4.817861
522.181851	8000.444417	12.544051	-0.101939	4.817860
522.443313	8000.391267	12.549056	-0.101987	4.817843
522.472942	8000.451788	12.554061	-0.101993	4.817861
522.532071	8000.436827	12.559066	-0.102004	4.817857
522.666401	8000.418737	12.564071	-0.102029	4.817851
522.799474	8000.400629	12.569075	-0.102053	4.817845
522.413410	8000.424558	12.574080	-0.101981	4.817853
522.651203	8000.397423	12.579085	-0.102026	4.817844
522.464635	8000.385232	12.584090	-0.101991	4.817842
522.189693	8000.427638	12.589095	-0.101940	4.817855
522.233827	8000.430383	12.594099	-0.101948	4.817856
521.810743	8000.432691	12.599104	-0.101869	4.817858
521.694690	8000.363536	12.604109	-0.101847	4.817838
521.978331	8000.470957	12.609114	-0.101900	4.817869
522.057741	8000.469995	12.614119	-0.101915	4.817868
522.218967	8000.507117	12.619123	-0.101945	4.817879
521.351245	8000.434464	12.624128	-0.101783	4.817861
521.609487	8000.432926	12.629133	-0.101831	4.817859
521.866890	8000.476711	12.634138	-0.101879	4.817871
521.872767	8000.361877	12.639143	-0.101880	4.817837
521.649958	8000.509411	12.644147	-0.101839	4.817882
521.648809	8000.500958	12.649152	-0.101839	4.817879
521.571265	8000.253135	12.654157	-0.101824	4.817806
521.660040	8000.420990	12.659162	-0.101841	4.817856
522.286972	8000.352043	12.664167	-0.101957	4.817832
522.094795	8000.505293	12.669171	-0.101922	4.817879
522.132944	8000.466834	12.674176	-0.101929	4.817867
522.594069	8000.434498	12.679181	-0.102014	4.817856
522.584106	8000.414319	12.684186	-0.102013	4.817850
522.538058	8000.389401	12.689191	-0.102004	4.817842
522.480058	8000.456034	12.694195	-0.101993	4.817862
521.824698	8000.353770	12.699200	-0.101871	4.817835
521.311869	8000.263062	12.704205	-0.101775	4.817810
521.260972	8000.261269	12.709210	-0.101766	4.817810
522.022006	8000.426199	12.714215	-0.101908	4.817856
522.164549	8000.516819	12.719219	-0.101934	4.817882
521.391042	8000.442366	12.724224	-0.101790	4.817863
521.365568	8000.153129	12.729229	-0.101785	4.817778
521.614121	8000.210488	12.734234	-0.101831	4.817793
521.009037	8000.055196	12.739239	-0.101719	4.817750
521.143689	8000.035001	12.744243	-0.101744	4.817743
521.870765	8000.351247	12.749248	-0.101879	4.817834
521.804929	8000.515813	12.754253	-0.101867	4.817883
521.487434	8000.380486	12.759258	-0.101808	4.817844
521.523741	8000.254498	12.764263	-0.101814	4.817807
521.797672	8000.336473	12.769267	-0.101865	4.817830
521.605413	8000.498155	12.774272	-0.101830	4.817879
521.518048	8000.226997	12.779277	-0.101813	4.817799
521.571107	8000.434397	12.784282	-0.101823	4.817860
521.803239	8000.512607	12.789287	-0.101866	4.817882
521.956603	8000.415722	12.794291	-0.101895	4.817853
522.065051	8000.486871	12.799296	-0.101915	4.817873
521.782424	8000.209722	12.804301	-0.101862	4.817793
521.751757	8000.401152	12.809306	-0.101857	4.817849
521.838993	8000.469886	12.814311	-0.101873	4.817869
522.065375	8000.439422	12.819315	-0.101915	4.817859
521.865891	8000.494518	12.824320	-0.101878	4.817876
522.063076	8000.422515	12.829325	-0.101915	4.817854
521.955830	8000.502140	12.834330	-0.101895	4.817878
522.256377	8000.420036	12.839335	-0.101950	4.817853
521.905654	8000.391764	12.844339	-0.101885	4.817846
521.893361	8000.483305	12.849344	-0.101883	4.817873
522.551391	8000.316761	12.854349	-0.102005	4.817821
522.179489	8000.501147	12.859354	-0.101936	4.817877
521.999740	8000.486945	12.864359	-0.101903	4.817874
522.007809	8000.404826	12.869363	-0.101904	4.817849
521.878845	8000.476756	12.874368	-0.101880	4.817871
521.677111	8000.426392	12.879373	-0.101842	4.817857
521.941577	8000.502962	12.884378	-0.101892	4.817879
522.036370	8000.373600	12.889383	-0.101909	4.817840
521.823719	8000.313590	12.894387	-0.101869	4.817823
521.966348	8000.499095	12.899392	-0.101896	4.817877
521.980202	8000.335880	12.904397	-0.101899	4.817829
522.098874	8000.390308	12.909402	-0.101921	4.817845
522.380610	8000.428120	12.914407	-0.101973	4.817855
522.431975	8000.505824	12.919411	-0.101983	4.817877
522.117639	8000.395843	12.924416	-0.101924	4.817846
522.310353	8000.493515	12.929421	-0.101960	4.817874
522.272465	8000.487693	12.934426	-0.101953	4.817873
522.087058	8000.488169	12.939431	-0.101918	4.817874
521.770315	8000.437195	12.944435	-0.101859	4.817860
522.020053	8000.485086	12.949440	-0.101906	4.817873
522.140433	8000.425677	12.954445	-0.101928	4.817855
522.191728	8000.508651	12.959450	-0.101938	4.817879
521.830885	8000.407486	12.964455	-0.101870	4.817851
521.999903	8000.224378	12.969459	-0.101902	4.817796
521.621326	8000.205193	12.974464	-0.101831	4.817792
522.034256	8000.095195	12.979469	-0.101908	4.817758
522.263963	8000.387386	12.984474	-0.101951	4.817843
522.480215	8000.451662	12.989479	-0.101991	4.817861
522.492742	8000.337978	12.994483	-0.101993	4.817827
522.817526	8000.427020	12.999488	-0.102054	4.817852
522.356949	8000.422458	13.004493	-0.101968	4.817853
522.603775	8000.449223	13.009498	-0.102014	4.817860
522.385037	8000.496660	13.014503	-0.101973	4.817875
522.194417	8000.429587	13.019507	-0.101938	4.817856
522.110332	8000.269171	13.024512	-0.101922	4.817809
522.176509	8000.276452	13.029517	-0.101934	4.817811
522.196248	8000.527654	13.034522	-0.101938	4.817885
522.190679	8000.359939	13.039527	-0.101937	4.817835
522.072316	8000.262285	13.044531	-0.101915	4.817807
522.208914	8000.389718	13.049536	-0.101940	4.817844
522.206250	8000.320094	13.054541	-0.101940	4.817823
522.232378	8000.437495	13.059546	-0.101944	4.817858
522.354856	8000.422396	13.064551	-0.101967	4.817853
522.614796	8000.459894	13.069555	-0.102016	4.817863
522.583425	8000.433079	13.074560	-0.102010	4.817855
522.343228	8000.399026	13.079565	-0.101965	4.817846
522.057317	8000.161891	13.084570	-0.101912	4.817777
522.040963	8000.245993	13.089575	-0.101908	4.817802
522.391722	8000.398665	13.094579	-0.101974	4.817846
522.387721	8000.456591	13.099584	-0.101973	4.817863
522.434924	8000.301237	13.104589	-0.101982	4.817817
522.606256	8000.370134	13.109594	-0.102014	4.817837
522.447397	8000.510161	13.114599	-0.101984	4.817879
522.198940	7999.886652	13.119603	-0.101937	4.817695
522.436307	8000.400349	13.124608	-0.101982	4.817846
522.375533	8000.301418	13.129613	-0.101971	4.817817
522.333806	8000.389371	13.134618	-0.101963	4.817843
522.431426	8000.290625	13.139623	-0.101981	4.817814
521.994003	8000.122990	13.144627	-0.101899	4.817766
521.976907	8000.493844	13.149632	-0.101896	4.817876
522.029906	8000.389180	13.154637	-0.101906	4.817845
522.481856	8000.209110	13.159642	-0.101990	4.817789
522.524050	8000.481724	13.164647	-0.101998	4.817870
522.462902	8000.310041	13.169651	-0.101987	4.817819
522.389399	8000.494529	13.174656	-0.101973	4.817874
522.101504	8000.315349	13.179661	-0.101919	4.817822
522.133569	8000.532993	13.184666	-0.101925	4.817887
522.469636	8000.332268	13.189671	-0.101988	4.817826
522.172603	8000.084431	13.194675	-0.101932	4.817754
521.626410	8000.004840	13.199680	-0.101830	4.817733
522.069685	7999.982783	13.204685	-0.101913	4.817724
521.927828	7999.980729	13.209690	-0.101886	4.817724
521.534634	8000.050946	13.214695	-0.101813	4.817747
521.964447	7999.952788	13.219699	-0.101893	4.817716
522.588813	8000.437295	13.224704	-0.102010	4.817857
522.221353	8000.161025	13.229709	-0.101941	4.817776
521.930991	8000.267519	13.234714	-0.101887	4.817809
521.827946	8000.239669	13.239719	-0.101868	4.817801
522.250235	8000.419732	13.244723	-0.101947	4.817853
521.645974	8000.089436	13.249728	-0.101834	4.817758
521.956776	8000.011697	13.254733	-0.101892	4.817733
521.989888	8000.064886	13.259738	-0.101898	4.817749
521.917636	8000.131310	13.264743	-0.101884	4.817769
521.890767	7999.941154	13.269747	-0.101879	4.817713
522.105824	8000.047578	13.274752	-0.101919	4.817743
522.112737	8000.130962	13.279757	-0.101920	4.817768
522.051992	8000.472719	13.284762	-0.101909	4.817869
522.312782	8000.446971	13.289767	-0.101958	4.817861
522.354426	8000.263071	13.294771	-0.101965	4.817806
522.232331	8000.513275	13.299776	-0.101943	4.817881
522.094202	8000.299363	13.304781	-0.101917	4.817818
522.088618	8000.121108	13.309786	-0.101916	4.817765
522.018676	8000.126420	13.314791	-0.101903	4.817767
522.054464	8000.118501	13.319795	-0.101909	4.817764
521.745836	8000.009663	13.324800	-0.101852	4.817734
521.819343	7999.898974	13.329805	-0.101865	4.817700
521.781104	8000.128244	13.334810	-0.101858	4.817768
521.854373	8000.205208	13.339815	-0.101872	4.817791
521.918188	7999.884581	13.344819	-0.101884	4.817696
521.712319	7999.833108	13.349824	-0.101845	4.817681
521.753564	7999.972861	13.354829	-0.101853	4.817723
521.804284	8000.100101	13.359834	-0.101862	4.817760
521.918598	8000.441226	13.364839	-0.101884	4.817861
522.217176	8000.277914	13.369843	-0.101939	4.817811
521.853683	8000.155629	13.374848	-0.101872	4.817776
522.189890	8000.184738	13.379853	-0.101934	4.817783
522.332356	8000.401869	13.384858	-0.101961	4.817847
522.273123	8000.521198	13.389863	-0.101950	4.817883
522.396767	8000.322670	13.394867	-0.101973	4.817823
522.840544	8000.306951	13.399872	-0.102055	4.817817
522.605476	8000.259266	13.404877	-0.102011	4.817804
522.691578	8000.337472	13.409882	-0.102028	4.817827
522.466907	8000.433321	13.414887	-0.101986	4.817856
522.593558	8000.363460	13.419891	-0.102009	4.817835
522.911906	8000.479821	13.424896	-0.102069	4.817868
522.328891	8000.232056	13.429901	-0.101960	4.817797
522.255243	8000.203577	13.434906	-0.101946	4.817789
523.127914	8000.359587	13.439911	-0.102109	4.817831
522.991293	8000.508372	13.444915	-0.102083	4.817876
523.027850	8000.460400	13.449920	-0.102090	4.817862
522.856587	8000.476895	13.454925	-0.102058	4.817867
522.976123	8000.463863	13.459930	-0.102080	4.817863
522.189214	8000.371289	13.464935	-0.101934	4.817839
522.382837	8000.104194	13.469939	-0.101969	4.817759
522.564369	8000.357736	13.474944	-0.102003	4.817833
523.297216	8000.312465	13.479949	-0.102140	4.817817
523.122947	8000.469139	13.484954	-0.102107	4.817864
523.262134	8000.365721	13.489959	-0.102133	4.817832
523.378763	8000.434883	13.494963	-0.102155	4.817852
523.358115	8000.398735	13.499968	-0.102151	4.817842
523.382208	8000.393809	13.504973	-0.102155	4.817840
523.309859	8000.443366	13.509978	-0.102142	4.817855
523.133240	8000.388090	13.514983	-0.102109	4.817840
523.544224	8000.429885	13.519987	-0.102186	4.817850
522.993805	8000.465139	13.524992	-0.102083	4.817863
523.097646	8000.460314	13.529997	-0.102102	4.817861
522.829087	8000.400545	13.535002	-0.102052	4.817845
522.807749	8000.426591	13.540007	-0.102048	4.817852
523.048638	8000.502823	13.545011	-0.102093	4.817874
522.883184	8000.476176	13.550016	-0.102062	4.817867
522.427571	8000.206006	13.555021	-0.101977	4.817789
522.756069	8000.251874	13.560026	-0.102038	4.817801
522.527944	8000.286524	13.565031	-0.101996	4.817812
523.034114	8000.423527	13.570035	-0.102090	4.817851
523.093462	8000.510837	13.575040	-0.102101	4.817876
522.975232	8000.435320	13.580045	-0.102079	4.817854
522.604556	8000.299220	13.585050	-0.102010	4.817816
522.544489	8000.342628	13.590055	-0.101999	4.817829
522.422834	8000.033016	13.595059	-0.101976	4.817738
522.191338	7999.937945	13.600064	-0.101933	4.817710
522.722496	8000.300916	13.605069	-0.102032	4.817816
523.164409	8000.368459	13.610074	-0.102114	4.817834
522.769475	8000.366957	13.615079	-0.102041	4.817835
522.544598	8000.401653	13.620083	-0.101999	4.817846
522.588483	8000.505607	13.625088	-0.102007	4.817877
522.700744	8000.340651	13.630093	-0.102028	4.817827
522.642254	8000.337693	13.635098	-0.102017	4.817827
522.092016	7999.947030	13.640103	-0.101914	4.817714
522.280191	7999.994028	13.645107	-0.101949	4.817727
522.357713	8000.233410	13.650112	-0.101964	4.817797
522.730396	8000.110179	13.655117	-0.102033	4.817759
522.508014	8000.105904	13.660122	-0.101991	4.817759
522.459745	8000.356121	13.665127	-0.101983	4.817833
522.627142	8000.381736	13.670131	-0.102014	4.817840
522.403189	8000.406957	13.675136	-0.101972	4.817848
522.138767	7999.853857	13.680141	-0.101922	4.817686
522.097867	8000.034594	13.685146	-0.101915	4.817739
522.192491	8000.253138	13.690151	-0.101933	4.817804
522.337099	8000.112901	13.695155	-0.101959	4.817762
522.104592	8000.007273	13.700160	-0.101916	4.817731
522.324208	8000.143283	13.705165	-0.101957	4.817771
522.565115	8000.199480	13.710170	-0.102002	4.817786
522.508318	8000.086903	13.715175	-0.101991	4.817753
522.517854	8000.229365	13.720179	-0.101993	4.817795
522.403848	8000.234038	13.725184	-0.101972	4.817797
522.641167	8000.162616	13.730189	-0.102016	4.817775
522.695285	8000.352113	13.735194	-0.102026	4.817831
522.214931	7999.845438	13.740199	-0.101936	4.817683
521.977705	7999.830409	13.745203	-0.101892	4.817679
522.111117	8000.164425	13.750208	-0.101917	4.817778
522.072674	7999.927713	13.755213	-0.101910	4.817708
522.180697	7999.955629	13.760218	-0.101930	4.817716
522.221604	8000.296745	13.765223	-0.101938	4.817817
522.326653	7999.961951	13.770227	-0.101957	4.817717
522.123956	8000.336443	13.775232	-0.101919	4.817829
522.244807	7999.902778	13.780237	-0.101942	4.817700
522.508121	7999.979327	13.785242	-0.101991	4.817721
522.592738	8000.362197	13.790247	-0.102007	4.817834
522.897767	8000.271723	13.795251	-0.102063	4.817806
522.627109	8000.227740	13.800256	-0.102013	4.817794
522.809621	8000.321048	13.805261	-0.102047	4.817821
522.751904	8000.291744	13.810266	-0.102036	4.817813
522.672221	8000.385474	13.815271	-0.102021	4.817841
522.776956	8000.215138	13.820275	-0.102041	4.817790
522.780062	8000.278438	13.825280	-0.102041	4.817809
522.413159	8000.366956	13.830285	-0.101973	4.817837
522.506498	8000.338785	13.835290	-0.101990	4.817828
522.994781	8000.376424	13.840295	-0.102081	4.817837
522.790355	8000.436720	13.845299	-0.102043	4.817856
522.510593	8000.194400	13.850304	-0.101991	4.817785
522.558407	7999.924142	13.855309	-0.101999	4.817705
522.366571	8000.084775	13.860314	-0.101964	4.817753
522.307482	8000.223081	13.865319	-0.101953	4.817794
522.896195	8000.280095	13.870323	-0.102062	4.817809
522.584515	8000.519122	13.875328	-0.102005	4.817881
522.475437	8000.193875	13.880333	-0.101984	4.817785
523.000653	8000.413386	13.885338	-0.102082	4.817848
523.025337	8000.464347	13.890343	-0.102086	4.817863
523.639088	8000.463744	13.895347	-0.102201	4.817860
523.641555	8000.470103	13.900352	-0.102201	4.817862
523.659133	8000.470355	13.905357	-0.102204	4.817862
523.740096	8000.385071	13.910362	-0.102219	4.817836
523.412704	8000.367675	13.915367	-0.102158	4.817832
523.909095	8000.424414	13.920371	-0.102251	4.817847
523.581028	8000.450235	13.925376	-0.102190	4.817856
523.972312	8000.416890	13.930381	-0.102262	4.817845
523.423957	8000.491182	13.935386	-0.102160	4.817869
523.410983	8000.433004	13.940391	-0.102158	4.817852
523.252437	8000.468661	13.945395	-0.102128	4.817863
523.391051	8000.424276	13.950400	-0.102154	4.817849
523.742137	8000.363990	13.955405	-0.102219	4.817830
523.479090	8000.390753	13.960410	-0.102170	4.817839
523.897860	8000.304035	13.965415	-0.102248	4.817812
524.127962	8000.348483	13.970419	-0.102291	4.817824
523.745448	8000.420960	13.975424	-0.102220	4.817847
523.710546	8000.400420	13.980429	-0.102213	4.817841
523.968733	8000.414700	13.985434	-0.102261	4.817844
524.004637	8000.388859	13.990439	-0.102268	4.817836
523.733939	8000.446087	13.995443	-0.102218	4.817854
523.876242	8000.395429	14.000448	-0.102244	4.817839
524.128028	8000.367444	14.005453	-0.102291	4.817829
523.571771	8000.498555	14.010458	-0.102187	4.817871
523.345552	8000.407768	14.015463	-0.102145	4.817845
523.462434	8000.524378	14.020467	-0.102167	4.817879
523.208888	8000.516486	14.025472	-0.102120	4.817877
523.491865	8000.439399	14.030477	-0.102172	4.817853
523.709443	8000.454145	14.035482	-0.102213	4.817857
523.119966	8000.465638	14.040487	-0.102103	4.817863
523.299549	8000.437661	14.045491	-0.102136	4.817854
523.128661	8000.481573	14.050496	-0.102105	4.817867
523.203021	8000.366673	14.055501	-0.102118	4.817833
523.417316	8000.511051	14.060506	-0.102158	4.817875
523.570380	8000.395182	14.065511	-0.102187	4.817840
523.298300	8000.353285	14.070515	-0.102136	4.817829
522.935052	8000.415498	14.075520	-0.102068	4.817849
523.101829	8000.393661	14.080525	-0.102099	4.817842
523.410476	8000.497233	14.085530	-0.102157	4.817871
523.009265	8000.417619	14.090535	-0.102082	4.817849
523.041720	8000.508756	14.095539	-0.102088	4.817876
523.510648	8000.462829	14.100544	-0.102175	4.817860
523.545250	8000.449621	14.105549	-0.102182	4.817856
523.532172	8000.406202	14.110554	-0.102179	4.817843
523.116819	8000.475041	14.115559	-0.102102	4.817866
523.680433	8000.487418	14.120563	-0.102207	4.817867
523.670496	8000.399763	14.125568	-0.102205	4.817841
523.805514	8000.379575	14.130573	-0.102230	4.817834
523.957904	8000.411301	14.135578	-0.102258	4.817843
523.824508	8000.387225	14.140583	-0.102234	4.817837
523.786822	8000.398274	14.145587	-0.102226	4.817840
523.977328	8000.408411	14.150592	-0.102262	4.817842
523.844795	8000.437064	14.155597	-0.102237	4.817851
523.945949	8000.361561	14.160602	-0.102256	4.817828
523.410196	8000.458177	14.165607	-0.102156	4.817859
523.908477	8000.439033	14.170611	-0.102249	4.817852
524.295360	8000.405624	14.175616	-0.102321	4.817840
523.830083	8000.411534	14.180621	-0.102234	4.817844
523.422959	8000.404581	14.185626	-0.102158	4.817843
523.333238	8000.462321	14.190631	-0.102142	4.817861
524.119901	8000.415724	14.195635	-0.102288	4.817844
523.693679	8000.475970	14.200640	-0.102209	4.817863
523.452444	8000.498831	14.205645	-0.102164	4.817871
523.680981	8000.466292	14.210650	-0.102206	4.817861
523.260941	8000.422251	14.215655	-0.102128	4.817849
523.485140	8000.461341	14.220659	-0.102170	4.817860
523.822906	8000.464122	14.225664	-0.102233	4.817859
523.704259	8000.447641	14.230669	-0.102211	4.817855
523.825660	8000.380865	14.235674	-0.102233	4.817835
524.074879	8000.442460	14.240679	-0.102279	4.817852
524.170892	8000.383752	14.245683	-0.102297	4.817834
523.622724	8000.449612	14.250688	-0.102195	4.817856
524.037796	8000.446132	14.255693	-0.102272	4.817853
524.147192	8000.456149	14.260698	-0.102293	4.817856
523.719495	8000.443625	14.265703	-0.102213	4.817854
523.589475	8000.488130	14.270707	-0.102189	4.817867
523.909943	8000.417912	14.275712	-0.102249	4.817845
523.500491	8000.402490	14.280717	-0.102172	4.817842
523.711826	8000.479351	14.285722	-0.102212	4.817864
523.686908	8000.465281	14.290727	-0.102207	4.817860
524.189263	8000.405078	14.295731	-0.102300	4.817840
523.747054	8000.481961	14.300736	-0.102218	4.817865
523.668729	8000.487150	14.305741	-0.102203	4.817867
524.097266	8000.379488	14.310746	-0.102283	4.817833
523.930116	8000.343326	14.315751	-0.102252	4.817823
524.110844	8000.377570	14.320755	-0.102286	4.817832
523.859205	8000.408716	14.325760	-0.102239	4.817843
523.474123	8000.466395	14.330765	-0.102167	4.817862
523.886955	8000.399623	14.335770	-0.102244	4.817840
523.630268	7999.477620	14.340775	-0.102195	4.817568

523.526627	7996.236721	14.345779	-0.102174	4.816609
523.559438	7990.642236	14.350784	-0.102176	4.814951
523.621898	7984.002075	14.355789	-0.102184	4.812983
524.054520	7976.753877	14.360794	-0.102259	4.810832
523.596947	7969.109308	14.365799	-0.102169	4.808567
523.935227	7961.375166	14.370803	-0.102227	4.806270
523.632776	7953.438412	14.375808	-0.102166	4.803915
523.747154	7945.542678	14.380813	-0.102182	4.801569
522.825356	7937.611086	14.385818	-0.102005	4.799215
523.061420	7929.574658	14.390823	-0.102044	4.796825
522.987012	7921.559236	14.395827	-0.102024	4.794441
523.199912	7913.583902	14.400832	-0.102059	4.792066
523.285422	7905.522854	14.405837	-0.102069	4.789665
523.037546	7897.607445	14.410842	-0.102018	4.787308
522.456642	7889.570652	14.415847	-0.101905	4.784914
522.373504	7881.579465	14.420851	-0.101884	4.782531
522.624433	7873.517658	14.425856	-0.101925	4.780125
522.282195	7865.496043	14.430861	-0.101856	4.777731
522.456335	7857.546970	14.435866	-0.101884	4.775356
522.245568	7849.583009	14.440871	-0.101839	4.772977
522.595988	7841.464130	14.445875	-0.101899	4.770548
522.442625	7833.506775	14.450880	-0.101865	4.768168
522.489743	7825.501283	14.455885	-0.101869	4.765772
523.096957	7817.442891	14.460890	-0.101977	4.763357
522.574523	7809.527260	14.465895	-0.101874	4.760987
522.650542	7801.558037	14.470899	-0.101883	4.758598
521.733086	7793.613582	14.475904	-0.101707	4.756219
522.011592	7785.442168	14.480909	-0.101754	4.753766
521.976555	7777.495563	14.485914	-0.101742	4.751380
522.055716	7769.452146	14.490919	-0.101751	4.748964
521.877322	7761.490541	14.495923	-0.101713	4.746572
521.801462	7753.456038	14.500928	-0.101693	4.744157
521.589098	7745.529329	14.505933	-0.101649	4.741773
521.767179	7737.502003	14.510938	-0.101677	4.739356
521.347789	7729.487467	14.515943	-0.101593	4.736944
521.117426	7721.478640	14.520947	-0.101545	4.734532
521.391829	7713.521271	14.525952	-0.101591	4.732132
522.041888	7705.332557	14.530957	-0.101707	4.729661
521.829380	7697.446884	14.535962	-0.101662	4.727282
521.472053	7689.410220	14.540967	-0.101590	4.724857
521.507387	7681.463139	14.545971	-0.101591	4.722456
521.648905	7673.433000	14.550976	-0.101613	4.720029
521.632861	7665.479238	14.555981	-0.101604	4.717624
521.651881	7657.492618	14.560986	-0.101603	4.715208
521.736561	7649.399114	14.565991	-0.101613	4.712758
521.228212	7641.441396	14.570995	-0.101513	4.710349
521.260442	7633.482722	14.576000	-0.101514	4.707938
521.390439	7625.435981	14.581005	-0.101533	4.705498
521.305072	7617.482816	14.586010	-0.101512	4.703086
520.911745	7609.492124	14.591015	-0.101433	4.700662
521.972041	7601.386233	14.596019	-0.101625	4.698200
521.876893	7593.413479	14.601024	-0.101602	4.695778
521.263147	7585.478543	14.606029	-0.101483	4.693367
521.508987	7577.463276	14.611034	-0.101524	4.690929
521.420358	7569.394323	14.616039	-0.101502	4.688474
521.123017	7561.479567	14.621043	-0.101441	4.686066
521.188643	7553.425821	14.626048	-0.101448	4.683613
521.287660	7545.427607	14.631053	-0.101461	4.681175
521.095622	7537.457155	14.636058	-0.101420	4.678745
521.261214	7529.495085	14.641063	-0.101446	4.676316
521.159679	7521.460658	14.646067	-0.101422	4.673864
520.721215	7513.431645	14.651072	-0.101335	4.671413
520.558653	7505.407705	14.656077	-0.101299	4.668962
520.582957	7497.438503	14.661082	-0.101299	4.666526
520.063917	7489.376413	14.666087	-0.101197	4.664060
519.823938	7481.510049	14.671091	-0.101147	4.661653
520.158675	7473.395997	14.676096	-0.101204	4.659169
520.368557	7465.474460	14.681101	-0.101238	4.656742
520.421178	7457.438647	14.686106	-0.101242	4.654279
520.281073	7449.421114	14.691111	-0.101211	4.651820
520.165589	7441.360094	14.696115	-0.101184	4.649347
520.195777	7433.401125	14.701120	-0.101185	4.646904
519.741950	7425.374958	14.706125	-0.101095	4.644439
519.704339	7417.490480	14.711130	-0.101083	4.642016
519.730017	7409.382767	14.716135	-0.101082	4.639523
519.359468	7401.455970	14.721139	-0.101008	4.637084
518.963870	7393.440214	14.726144	-0.100929	4.634617
518.975133	7385.394243	14.731149	-0.100926	4.632139
519.437239	7377.342156	14.736154	-0.101006	4.629658
518.806501	7369.411568	14.741159	-0.100884	4.627213
519.106108	7361.364044	14.746163	-0.100934	4.624730
519.026891	7353.420310	14.751168	-0.100914	4.622279
518.953856	7345.417142	14.756173	-0.100896	4.619807
519.027268	7337.429169	14.761178	-0.100904	4.617339
518.797582	7329.391476	14.766183	-0.100856	4.614855
518.344021	7321.424255	14.771187	-0.100766	4.612390
518.327093	7313.363689	14.776192	-0.100758	4.609896
518.666803	7305.310674	14.781197	-0.100816	4.607402
518.593030	7297.353643	14.786202	-0.100797	4.604937
518.365614	7289.371132	14.791207	-0.100749	4.602463
518.344368	7281.406483	14.796211	-0.100740	4.599993
518.199426	7273.438477	14.801216	-0.100708	4.597520
518.270618	7265.336366	14.806221	-0.100716	4.595005
518.306451	7257.381473	14.811226	-0.100717	4.592533
518.160382	7249.316057	14.816231	-0.100685	4.590026
518.375011	7241.325948	14.821235	-0.100719	4.587542
518.369057	7233.288846	14.826240	-0.100713	4.585041
518.384430	7225.326227	14.831245	-0.100711	4.582562
518.435688	7217.305631	14.836250	-0.100715	4.580064
518.030532	7209.385700	14.841255	-0.100634	4.577595
518.119102	7201.303621	14.846259	-0.100646	4.575075
518.579312	7193.269081	14.851264	-0.100726	4.572569
517.935101	7185.325636	14.856269	-0.100601	4.570088
518.121646	7177.350206	14.861274	-0.100630	4.567598
517.826701	7169.274947	14.866279	-0.100570	4.565074
518.045503	7161.364946	14.871283	-0.100606	4.562601
518.079490	7153.308642	14.876288	-0.100607	4.560080
517.610139	7145.376613	14.881293	-0.100514	4.557596
517.539320	7137.308995	14.886298	-0.100496	4.555069
517.152893	7129.337636	14.891303	-0.100418	4.552571
517.513494	7121.274098	14.896307	-0.100480	4.550043
517.688490	7113.259994	14.901312	-0.100508	4.547529
517.852442	7105.182728	14.906317	-0.100533	4.544994
517.913758	7097.312413	14.911322	-0.100539	4.542522
517.774744	7089.222437	14.916327	-0.100508	4.539980
517.649233	7081.331512	14.921331	-0.100479	4.537498
517.409036	7073.317900	14.926336	-0.100429	4.534977
517.587442	7065.272679	14.931341	-0.100457	4.532445
518.284867	7057.174003	14.936346	-0.100582	4.529896
517.691353	7049.267052	14.941351	-0.100466	4.527403
517.775026	7041.251817	14.946355	-0.100477	4.524876
517.793348	7033.329676	14.951360	-0.100475	4.522377
517.193553	7025.300927	14.956365	-0.100358	4.519841
517.239418	7017.339047	14.961370	-0.100361	4.517326
516.951557	7009.305779	14.966375	-0.100302	4.514787
516.948700	7001.311873	14.971379	-0.100296	4.512259
516.865823	6993.261101	14.976384	-0.100276	4.509712
517.072702	6985.224787	14.981389	-0.100309	4.507169
517.067124	6977.200067	14.986394	-0.100303	4.504627
517.001847	6969.240596	14.991399	-0.100285	4.502105
517.167572	6961.195528	14.996403	-0.100311	4.499554
517.193890	6953.204697	15.001408	-0.100311	4.497019
517.154475	6945.191573	15.006413	-0.100298	4.494475
516.999481	6937.251141	15.011418	-0.100264	4.491953
516.888787	6929.138931	15.016423	-0.100238	4.489374
517.101625	6921.256337	15.021427	-0.100272	4.486869
516.481602	6913.198673	15.026432	-0.100152	4.484303
516.805449	6905.216788	15.031437	-0.100207	4.481763
516.945988	6897.226868	15.036442	-0.100228	4.479218
517.029264	6889.190254	15.041447	-0.100238	4.476658
516.987967	6881.205798	15.046451	-0.100225	4.474111
516.889890	6873.246208	15.051456	-0.100202	4.471571
516.751604	6865.143114	15.056461	-0.100170	4.468984
516.528641	6857.235452	15.061466	-0.100124	4.466457
516.417659	6849.175587	15.066471	-0.100098	4.463880
516.751748	6841.216815	15.071475	-0.100155	4.461336
516.319512	6833.219441	15.076480	-0.100069	4.458775
516.033276	6825.216015	15.081485	-0.100010	4.456212
516.680767	6817.117294	15.086490	-0.100126	4.453620
516.454736	6809.172954	15.091495	-0.100078	4.451072
516.055611	6801.192004	15.096499	-0.099999	4.448511
515.822518	6793.244475	15.101504	-0.099950	4.445959
515.774014	6785.133596	15.106509	-0.099936	4.443354
515.810386	6777.189405	15.111514	-0.099937	4.440802
515.656533	6769.192517	15.116519	-0.099904	4.438231
515.777591	6761.184395	15.121523	-0.099921	4.435655
515.506885	6753.189989	15.126528	-0.099865	4.433081
515.210028	6745.166841	15.131533	-0.099805	4.430496
515.892141	6737.071618	15.136538	-0.099926	4.427891
515.650897	6729.162537	15.141543	-0.099876	4.425339
515.756150	6721.134342	15.146547	-0.099891	4.422750
515.125268	6713.215025	15.151552	-0.099768	4.420190
515.415429	6705.141900	15.156557	-0.099817	4.417584
515.447259	6697.102977	15.161562	-0.099817	4.414986
515.768281	6689.089819	15.166567	-0.099872	4.412397
515.565110	6681.111672	15.171571	-0.099829	4.409814
515.214564	6673.158258	15.176576	-0.099758	4.407238
514.932031	6665.099550	15.181581	-0.099700	4.404625
514.958371	6657.192277	15.186586	-0.099700	4.402063
514.768180	6649.128056	15.191591	-0.099659	4.399446
515.138562	6641.159311	15.196595	-0.099723	4.396862
515.493173	6633.040653	15.201600	-0.099784	4.394228
515.708372	6625.082107	15.206605	-0.099819	4.391644
515.444925	6617.109476	15.211610	-0.099764	4.389050
515.063333	6609.119005	15.216615	-0.099688	4.386449
515.250626	6601.094531	15.221619	-0.099718	4.383838
514.727263	6593.249771	15.226624	-0.099615	4.381280
514.878275	6585.111935	15.231629	-0.099638	4.378629
514.444198	6577.236726	15.236634	-0.099552	4.376058
514.551592	6569.195588	15.241639	-0.099567	4.373436
514.757210	6561.160095	15.246643	-0.099600	4.370814
514.485501	6553.212787	15.251648	-0.099544	4.368216
514.539742	6545.147980	15.256653	-0.099549	4.365580
514.578608	6537.179969	15.261658	-0.099551	4.362975
514.502921	6529.185763	15.266663	-0.099531	4.360358
514.669333	6521.214078	15.271667	-0.099557	4.357749
514.551077	6513.211354	15.276672	-0.099530	4.355126
514.264532	6505.176244	15.281677	-0.099471	4.352490
515.142788	6497.059574	15.286682	-0.099629	4.349834
514.517490	6489.161595	15.291687	-0.099508	4.347237
514.648978	6481.092929	15.296691	-0.099527	4.344588
514.331300	6473.210246	15.301696	-0.099463	4.341995
514.515010	6465.176701	15.306701	-0.099492	4.339355
514.400862	6457.227871	15.311706	-0.099465	4.336739
514.234078	6449.182728	15.316711	-0.099429	4.334089
514.356505	6441.187924	15.321715	-0.099446	4.331456
514.047277	6433.241258	15.326720	-0.099384	4.328834
514.135708	6425.168965	15.331725	-0.099395	4.326172
514.178058	6417.178369	15.336730	-0.099397	4.323535
514.285657	6409.198624	15.341735	-0.099412	4.320901
514.562603	6401.173304	15.346739	-0.099458	4.318251
514.505723	6393.210086	15.351744	-0.099443	4.315618
514.316657	6385.138998	15.356749	-0.099402	4.312946
514.668171	6377.141535	15.361754	-0.099462	4.310302
514.419148	6369.149807	15.366759	-0.099411	4.307652
514.206889	6361.148048	15.371763	-0.099366	4.304998
514.008859	6353.182950	15.376768	-0.099324	4.302355
514.001475	6345.120126	15.381773	-0.099317	4.299679
513.687105	6337.220663	15.386778	-0.099254	4.297053
514.124074	6329.104606	15.391783	-0.099330	4.294360
514.288593	6321.089811	15.396787	-0.099355	4.291697
513.688560	6313.129270	15.401792	-0.099238	4.289043
513.885274	6305.122643	15.406797	-0.099269	4.286379
513.848663	6297.176850	15.411802	-0.099257	4.283732
513.801960	6289.165102	15.416807	-0.099243	4.281061
513.343700	6281.178026	15.421811	-0.099153	4.278393
513.668684	6273.200799	15.426816	-0.099208	4.275734
513.758867	6265.091913	15.431821	-0.099220	4.273027
513.962227	6257.087724	15.436826	-0.099252	4.270354
513.798040	6249.123983	15.441831	-0.099216	4.267690
513.702096	6241.154034	15.446835	-0.099193	4.265022
513.870973	6233.166672	15.451840	-0.099220	4.262350
513.958664	6225.111119	15.456845	-0.099231	4.259652
513.375653	6217.212183	15.461850	-0.099117	4.256999
513.100077	6209.156897	15.466855	-0.099060	4.254294
513.710307	6201.105155	15.471859	-0.099169	4.251598
513.367668	6193.123473	15.476864	-0.099100	4.248914
513.045271	6185.166813	15.481869	-0.099034	4.246237
512.981206	6177.145430	15.486874	-0.099017	4.243538
512.727056	6169.196099	15.491879	-0.098965	4.240861
512.555234	6161.213264	15.496883	-0.098927	4.238171
512.712561	6153.112562	15.501888	-0.098951	4.235444
512.594008	6145.105071	15.506893	-0.098924	4.232743
513.063056	6137.075416	15.511898	-0.099006	4.230039
512.880877	6129.087517	15.516903	-0.098967	4.227341
512.597151	6121.130139	15.521907	-0.098909	4.224650
513.058259	6113.093662	15.526912	-0.098989	4.221938
512.935169	6105.064908	15.531917	-0.098961	4.219222
512.800987	6097.166229	15.536922	-0.098931	4.216547
512.953556	6089.047816	15.541927	-0.098954	4.213799
512.790899	6081.140941	15.546931	-0.098919	4.211118
512.782470	6073.092449	15.551936	-0.098912	4.208389
512.889678	6065.089580	15.556941	-0.098927	4.205675
512.982870	6057.153888	15.561946	-0.098939	4.202981
512.084370	6049.212703	15.566951	-0.098766	4.200273
512.178902	6041.238642	15.571955	-0.098779	4.197563
512.385233	6033.119191	15.576960	-0.098812	4.194803
511.916701	6025.102784	15.581965	-0.098719	4.192069
511.917110	6017.074181	15.586970	-0.098714	4.189334
511.745087	6009.088715	15.591975	-0.098677	4.186610
511.146996	6001.142257	15.596979	-0.098560	4.183893
511.295157	5993.115293	15.601984	-0.098582	4.181155
511.220509	5985.093901	15.606989	-0.098563	4.178414
511.564618	5977.116264	15.611994	-0.098622	4.175692
511.709190	5969.021972	15.616999	-0.098644	4.172926
511.990575	5961.001162	15.622003	-0.098691	4.170184
511.823591	5953.073318	15.627008	-0.098655	4.167467
511.630516	5945.039615	15.632013	-0.098613	4.164712
511.323231	5937.166477	15.637018	-0.098551	4.162009
511.074974	5929.165490	15.642023	-0.098499	4.159261
511.581512	5921.158174	15.647027	-0.098589	4.156518
511.405179	5913.161589	15.652032	-0.098550	4.153768
511.367835	5905.110852	15.657037	-0.098538	4.151000
511.075430	5897.148325	15.662042	-0.098479	4.148257
510.389081	5889.222911	15.667047	-0.098346	4.145520
510.428749	5881.190103	15.672051	-0.098348	4.142753
510.526567	5873.130614	15.677056	-0.098361	4.139976
510.981083	5865.091217	15.682061	-0.098440	4.137209
510.493154	5857.137631	15.687066	-0.098344	4.134457
510.327890	5849.197242	15.692071	-0.098308	4.131712
510.469260	5841.119641	15.697075	-0.098329	4.128922
510.249937	5833.145127	15.702080	-0.098283	4.126161
510.431296	5825.079529	15.707085	-0.098311	4.123372
511.124200	5817.089721	15.712090	-0.098435	4.120614
510.255175	5809.200596	15.717095	-0.098268	4.117868
510.225690	5801.164734	15.722099	-0.098257	4.115081
510.287148	5793.164052	15.727104	-0.098264	4.112305
510.310473	5785.100157	15.732109	-0.098263	4.109505
510.138168	5777.120432	15.737114	-0.098225	4.106729
510.348785	5769.034052	15.742119	-0.098259	4.103920
510.260354	5761.192859	15.747123	-0.098238	4.101190
510.105850	5753.172264	15.752128	-0.098204	4.098395
510.234060	5745.082233	15.757133	-0.098222	4.095578
510.147845	5737.131705	15.762138	-0.098201	4.092804
509.857639	5729.154658	15.767143	-0.098142	4.090016
509.813340	5721.159721	15.772147	-0.098128	4.087224
509.963244	5713.114069	15.777152	-0.098151	4.084415
510.175956	5705.102545	15.782157	-0.098185	4.081617
510.092689	5697.118513	15.787162	-0.098164	4.078822
509.809656	5689.202686	15.792167	-0.098106	4.076046
510.255206	5681.089985	15.797171	-0.098184	4.073210
510.338034	5673.091463	15.802176	-0.098194	4.070407
510.191683	5665.092089	15.807181	-0.098162	4.067598
509.846656	5657.178735	15.812186	-0.098092	4.064814
509.941579	5649.137620	15.817191	-0.098105	4.061991
509.616806	5641.126244	15.822195	-0.098039	4.059169
509.910709	5633.181793	15.827200	-0.098089	4.056378
509.356476	5625.174733	15.832205	-0.097980	4.053551
509.607431	5617.150078	15.837210	-0.098022	4.050727
509.600543	5609.125340	15.842215	-0.098015	4.047898
509.580176	5601.149272	15.847219	-0.098006	4.045083
509.551596	5593.154382	15.852224	-0.097995	4.042260
509.428527	5585.089772	15.857229	-0.097967	4.039409
509.726910	5577.167572	15.862234	-0.098018	4.036612
509.103464	5569.174500	15.867239	-0.097896	4.033774
509.538518	5561.051811	15.872243	-0.097972	4.030905
509.064599	5553.152627	15.877248	-0.097878	4.028099
508.977370	5545.117591	15.882253	-0.097857	4.025248
508.844755	5537.205571	15.887258	-0.097827	4.022439
508.744668	5529.131540	15.892263	-0.097803	4.019570
508.790653	5521.165554	15.897267	-0.097806	4.016741
508.741394	5513.165658	15.902272	-0.097792	4.013895
508.813639	5505.151828	15.907277	-0.097800	4.011045
508.229379	5497.220520	15.912282	-0.097686	4.008211
508.616608	5489.079119	15.917287	-0.097753	4.005316
508.297714	5481.214468	15.922291	-0.097689	4.002506
508.030939	5473.189492	15.927296	-0.097634	3.999638
507.920754	5465.216331	15.932301	-0.097608	3.996789
508.135717	5457.190745	15.937306	-0.097643	3.993925
507.830731	5449.214713	15.942311	-0.097581	3.991067
507.635054	5441.221007	15.947315	-0.097539	3.988203
507.882358	5433.116949	15.952320	-0.097580	3.985305
508.100073	5425.128087	15.957325	-0.097615	3.982445
508.119525	5417.152703	15.962330	-0.097613	3.979585
508.263099	5409.163997	15.967335	-0.097635	3.976721
507.839600	5401.215522	15.972339	-0.097551	3.973858
507.874771	5393.225386	15.977344	-0.097552	3.970987
507.468217	5385.195866	15.982349	-0.097471	3.968092
507.491248	5377.231008	15.987354	-0.097470	3.965225
507.163483	5369.251120	15.992359	-0.097404	3.962345
507.563109	5361.160584	15.997363	-0.097473	3.959435
507.813460	5353.174103	16.002368	-0.097514	3.956559
507.616506	5345.170740	16.007373	-0.097472	3.953666
506.912974	5337.289452	16.012378	-0.097336	3.950806
506.993884	5329.225320	16.017383	-0.097346	3.947892
506.632358	5321.220545	16.022387	-0.097273	3.944989
506.550662	5313.251573	16.027392	-0.097253	3.942102
506.806943	5305.127420	16.032397	-0.097295	3.939163
506.640234	5297.255498	16.037402	-0.097259	3.936305
506.531764	5289.226414	16.042407	-0.097234	3.933390
506.358010	5281.211859	16.047411	-0.097196	3.930476
506.322005	5273.242572	16.052416	-0.097184	3.927579
506.424923	5265.132961	16.057421	-0.097198	3.924632
506.575402	5257.222425	16.062426	-0.097221	3.921755
506.394271	5249.189325	16.067431	-0.097182	3.918826
506.193137	5241.242993	16.072435	-0.097139	3.915925
505.942765	5233.277003	16.077440	-0.097087	3.913015
506.216945	5225.173889	16.082445	-0.097133	3.910062
506.323894	5217.170238	16.087450	-0.097148	3.907140
506.118498	5209.168695	16.092455	-0.097104	3.904211
506.226630	5201.216190	16.097459	-0.097119	3.901303
505.746155	5193.303728	16.102464	-0.097025	3.898397
505.483872	5185.297901	16.107469	-0.096970	3.895458
505.302704	5177.365336	16.112474	-0.096932	3.892545
505.374051	5169.249057	16.117479	-0.096939	3.889568
505.751096	5161.232786	16.122483	-0.097004	3.886632
505.348143	5153.252313	16.127488	-0.096924	3.883691
505.575787	5145.226508	16.132493	-0.096961	3.880743
505.873596	5137.243544	16.137498	-0.097012	3.877811
505.844717	5129.274376	16.142503	-0.097001	3.874874
505.622280	5121.141686	16.147507	-0.096954	3.871872
505.527843	5113.145320	16.152512	-0.096931	3.868919
505.239818	5105.188731	16.157517	-0.096872	3.865976
505.032477	5097.233814	16.162522	-0.096829	3.863032
505.512072	5089.200028	16.167527	-0.096913	3.860071
505.346132	5081.243191	16.172531	-0.096877	3.857123
505.404079	5073.227601	16.177536	-0.096882	3.854155
505.756151	5065.205674	16.182541	-0.096942	3.851190
505.966221	5057.200397	16.187546	-0.096976	3.848225
505.487922	5049.280075	16.192551	-0.096882	3.845274
505.388956	5041.319922	16.197555	-0.096858	3.842315
505.597705	5033.243314	16.202560	-0.096892	3.839317
505.244943	5025.324464	16.207565	-0.096821	3.836362
505.647033	5017.293538	16.212570	-0.096891	3.833381
505.639594	5009.246446	16.217575	-0.096884	3.830382
505.928755	5001.219324	16.222579	-0.096933	3.827394
505.062860	4993.378835	16.227584	-0.096766	3.824449
504.900107	4985.364786	16.232589	-0.096731	3.821452
504.769696	4977.376901	16.237594	-0.096701	3.818463
504.991029	4969.267769	16.242599	-0.096737	3.815434
505.018530	4961.268167	16.247603	-0.096737	3.812439
504.894274	4953.303029	16.252608	-0.096708	3.809452
504.410382	4945.364006	16.257613	-0.096613	3.806464
504.527227	4937.332259	16.262618	-0.096630	3.803452
504.255569	4929.340144	16.267623	-0.096574	3.800444
504.628958	4921.305635	16.272627	-0.096638	3.797432
504.553583	4913.326880	16.277632	-0.096619	3.794429
504.481765	4905.305362	16.282637	-0.096600	3.791407
504.046497	4897.381140	16.287642	-0.096514	3.788411
503.961158	4889.374984	16.292647	-0.096493	3.785390
503.953491	4881.318413	16.297651	-0.096486	3.782349
504.562148	4873.251942	16.302656	-0.096594	3.779316
503.809745	4865.410973	16.307661	-0.096449	3.776335
504.094426	4857.346599	16.312666	-0.096497	3.773291
503.786302	4849.383906	16.317671	-0.096434	3.770268
503.592938	4841.418127	16.322675	-0.096393	3.767245
503.823986	4833.332772	16.327680	-0.096431	3.764185
503.751554	4825.366634	16.332685	-0.096412	3.761159
503.700385	4817.388355	16.337690	-0.096397	3.758128
503.731260	4809.367867	16.342695	-0.096398	3.755079
503.560118	4801.385515	16.347699	-0.096360	3.752038
503.436705	4793.404233	16.352704	-0.096332	3.748996
503.604705	4785.397859	16.357709	-0.096358	3.745949
503.412780	4777.424977	16.362714	-0.096317	3.742903
503.314843	4769.395433	16.367719	-0.096294	3.739836
503.714740	4761.377345	16.372723	-0.096363	3.736783
503.729071	4753.397800	16.377728	-0.096360	3.733732
503.802531	4745.366317	16.382733	-0.096369	3.730661
503.573300	4737.453101	16.387738	-0.096321	3.727625
503.392583	4729.421971	16.392743	-0.096282	3.724542
503.469087	4721.433703	16.397747	-0.096291	3.721480
503.616826	4713.437575	16.402752	-0.096313	3.718414
503.610783	4705.441003	16.407757	-0.096307	3.715341
503.710425	4697.414084	16.412762	-0.096320	3.712257
503.021184	4689.446601	16.417767	-0.096187	3.709173
503.085215	4681.414390	16.422771	-0.096193	3.706080
503.386455	4673.409562	16.427776	-0.096244	3.703002
503.107086	4665.419941	16.432781	-0.096187	3.699912
503.178677	4657.458169	16.437786	-0.096195	3.696840
502.663728	4649.484887	16.442791	-0.096094	3.693745
502.968748	4641.432868	16.447795	-0.096145	3.690638
502.765764	4633.461170	16.452800	-0.096102	3.687547
502.194454	4625.497743	16.457805	-0.095991	3.684446
502.253045	4617.552581	16.462810	-0.095996	3.681367
502.139289	4609.506741	16.467815	-0.095970	3.678241
502.242471	4601.471513	16.472819	-0.095984	3.675122
502.886194	4593.401365	16.477824	-0.096099	3.672002
502.579468	4585.428499	16.482829	-0.096036	3.668891
502.747431	4577.447593	16.487834	-0.096062	3.665788
502.785312	4569.461511	16.492839	-0.096064	3.662676
502.327092	4561.538040	16.497843	-0.095973	3.659573
502.323922	4553.558837	16.502848	-0.095968	3.656457
502.391239	4545.500892	16.507853	-0.095975	3.653310
502.445331	4537.553716	16.512858	-0.095980	3.650204
502.061486	4529.563330	16.517863	-0.095903	3.647065
502.225019	4521.485936	16.522867	-0.095928	3.643905
502.774924	4513.528439	16.527872	-0.096025	3.640800
502.496265	4505.515722	16.532877	-0.095968	3.637648
502.452271	4497.598396	16.537882	-0.095955	3.634537
501.832160	4489.655607	16.542887	-0.095834	3.631397
501.718579	4481.604725	16.547891	-0.095808	3.628226
501.678779	4473.611950	16.552896	-0.095795	3.625077
502.033761	4465.552061	16.557901	-0.095856	3.621910
501.994229	4457.572377	16.562906	-0.095843	3.618761
501.514014	4449.630480	16.567911	-0.095749	3.615612
501.910561	4441.551336	16.572915	-0.095817	3.612430
501.921623	4433.562950	16.577920	-0.095814	3.609271
501.161357	4425.663345	16.582925	-0.095667	3.606121
501.096507	4417.641815	16.587930	-0.095650	3.602941
501.403238	4409.579932	16.592935	-0.095702	3.599752
501.507698	4401.613702	16.597939	-0.095716	3.596593
501.688191	4393.615883	16.602944	-0.095744	3.593421
501.643557	4385.596815	16.607949	-0.095731	3.590231
501.315748	4377.689602	16.612954	-0.095665	3.587074
500.925600	4369.673455	16.617959	-0.095587	3.583870
501.475926	4361.625723	16.622963	-0.095684	3.580677
501.389732	4353.684453	16.627968	-0.095663	3.577505
501.134376	4345.645638	16.632973	-0.095610	3.574287
501.148953	4337.715860	16.637978	-0.095607	3.571117
501.053769	4329.678094	16.642983	-0.095584	3.567898
500.812777	4321.667112	16.647987	-0.095534	3.564682
501.271548	4313.654570	16.652992	-0.095614	3.561484
501.389161	4305.628017	16.657997	-0.095631	3.558267
501.695499	4297.678367	16.663002	-0.095683	3.555084
500.830139	4289.745096	16.668007	-0.095516	3.551869
500.599604	4281.725528	16.673011	-0.095468	3.548636
501.163581	4273.639830	16.678016	-0.095568	3.545397
501.175491	4265.678429	16.683021	-0.095565	3.542188
500.393220	4257.793408	16.688026	-0.095414	3.538983
500.342012	4249.796542	16.693031	-0.095399	3.535753
500.058112	4241.814068	16.698035	-0.095341	3.532518
500.065618	4233.748731	16.703040	-0.095337	3.529255
500.525088	4225.686038	16.708045	-0.095418	3.526005
500.715631	4217.706044	16.713050	-0.095448	3.522777
500.707937	4209.717116	16.718055	-0.095441	3.519536
500.547594	4201.792766	16.723059	-0.095406	3.516313
500.496056	4193.800477	16.728064	-0.095391	3.513063
500.670893	4185.741926	16.733069	-0.095419	3.509791
500.683995	4177.799285	16.738074	-0.095416	3.506558
500.789758	4169.760214	16.743079	-0.095430	3.503285
500.524198	4161.822097	16.748083	-0.095376	3.500038
500.521948	4153.834777	16.753088	-0.095370	3.496777
500.108761	4145.859164	16.758093	-0.095288	3.493504
500.327593	4137.835770	16.763098	-0.095323	3.490229
499.519996	4129.941024	16.768103	-0.095168	3.486970
499.521255	4121.879186	16.773107	-0.095163	3.483666
499.468410	4113.945707	16.778112	-0.095148	3.480410
499.165151	4105.940175	16.783117	-0.095086	3.477113
499.446132	4097.900047	16.788122	-0.095133	3.473818
499.445457	4089.866570	16.793127	-0.095128	3.470513
499.614833	4081.841434	16.798131	-0.095154	3.467214
499.609008	4073.827427	16.803136	-0.095147	3.463910
499.277410	4065.939747	16.808141	-0.095081	3.460645
499.368215	4057.907479	16.813146	-0.095092	3.457331
499.398931	4049.872671	16.818151	-0.095093	3.454011
499.086806	4041.960291	16.823155	-0.095029	3.450726
498.853832	4033.963978	16.828160	-0.094981	3.447407
498.745377	4025.930644	16.833165	-0.094955	3.444073
498.491565	4018.019365	16.838170	-0.094903	3.440781
498.649994	4009.993163	16.843175	-0.094927	3.437453
498.787161	4001.948651	16.848179	-0.094947	3.434113
498.384484	3994.054071	16.853184	-0.094867	3.430814
498.323294	3985.989874	16.858189	-0.094850	3.427452
498.586837	3977.961993	16.863194	-0.094894	3.424114
498.605832	3970.012299	16.868199	-0.094893	3.420796
498.385901	3962.032018	16.873203	-0.094846	3.417455
498.192976	3954.060374	16.878208	-0.094805	3.414114
498.207184	3946.026316	16.883213	-0.094803	3.410751
498.387684	3938.026400	16.888218	-0.094831	3.407406
498.166931	3930.026438	16.893223	-0.094785	3.404042
497.877822	3922.124996	16.898227	-0.094726	3.400714
498.362491	3914.033713	16.903232	-0.094811	3.397331
498.140160	3906.035519	16.908237	-0.094764	3.393958
498.871169	3897.952393	16.913242	-0.094895	3.390581
498.380797	3890.052971	16.918247	-0.094798	3.387233
498.065852	3882.063029	16.923251	-0.094734	3.383851
498.439693	3874.093872	16.928256	-0.094799	3.380498
497.993330	3866.120964	16.933261	-0.094710	3.377111
497.831992	3858.151644	16.938266	-0.094675	3.373733
497.166910	3850.213222	16.943271	-0.094546	3.370345
497.110518	3842.200304	16.948275	-0.094530	3.366945
497.738080	3834.076699	16.953280	-0.094642	3.363520
497.438362	3826.152496	16.958285	-0.094581	3.360141
497.481273	3818.196314	16.963290	-0.094584	3.356759
497.713928	3810.115794	16.968295	-0.094622	3.353327
497.601193	3802.152704	16.973299	-0.094595	3.349928
497.723737	3794.154464	16.978304	-0.094613	3.346520
497.549311	3786.196973	16.983309	-0.094575	3.343115
497.505544	3778.229608	16.988314	-0.094562	3.339707
497.256927	3770.256389	16.993319	-0.094510	3.336285
497.351698	3762.258932	16.998323	-0.094523	3.332863
497.538098	3754.235338	17.003328	-0.094552	3.329429
497.190872	3746.261502	17.008333	-0.094482	3.325992
497.067925	3738.311699	17.013338	-0.094454	3.322571
497.070772	3730.290021	17.018343	-0.094449	3.319121
496.542809	3722.397310	17.023347	-0.094346	3.315701
496.856454	3714.321082	17.028352	-0.094399	3.312232
496.844123	3706.294721	17.033357	-0.094392	3.308768
496.994718	3698.291013	17.038362	-0.094414	3.305316
496.960423	3690.297111	17.043367	-0.094403	3.301858
497.130148	3682.262180	17.048371	-0.094429	3.298386
496.821126	3674.391300	17.053376	-0.094366	3.294963
496.332890	3666.420571	17.058381	-0.094270	3.291486
496.361735	3658.381315	17.063386	-0.094270	3.287996
496.588972	3650.351887	17.068391	-0.094307	3.284514
496.779060	3642.367242	17.073395	-0.094337	3.281047
496.215410	3634.505756	17.078400	-0.094227	3.277600
496.148347	3626.457747	17.083405	-0.094210	3.274087
496.225995	3618.472296	17.088410	-0.094219	3.270604
495.635013	3610.515479	17.093415	-0.094104	3.267103
495.623151	3602.489796	17.098419	-0.094096	3.263591
495.481469	3594.518249	17.103424	-0.094064	3.260094
495.333840	3586.524568	17.108429	-0.094032	3.256583
495.453777	3578.492700	17.113434	-0.094049	3.253062
495.425690	3570.491768	17.118439	-0.094038	3.249545
495.522664	3562.493528	17.123443	-0.094051	3.246030
495.551453	3554.530118	17.128448	-0.094051	3.242525
495.823110	3546.459140	17.133453	-0.094097	3.238978
495.967629	3538.529703	17.138458	-0.094118	3.235484
495.341120	3530.603568	17.143463	-0.093996	3.231956
495.164549	3522.600268	17.148467	-0.093958	3.228409
495.018995	3514.627590	17.153472	-0.093926	3.224873
494.841578	3506.641406	17.158477	-0.093888	3.221325
495.029569	3498.597126	17.163482	-0.093917	3.217764
494.750762	3490.611625	17.168487	-0.093860	3.214204
494.743218	3482.594557	17.173491	-0.093854	3.210638
494.618266	3474.648760	17.178496	-0.093825	3.207095
494.834538	3466.578393	17.183501	-0.093860	3.203507
494.914044	3458.630753	17.188506	-0.093870	3.199964
494.761847	3450.684778	17.193511	-0.093836	3.196407
495.051130	3442.622949	17.198515	-0.093885	3.192814
495.237275	3434.612049	17.203520	-0.093914	3.189236
495.239454	3426.616675	17.208525	-0.093909	3.185652
495.339593	3418.672278	17.213530	-0.093923	3.182091
494.922228	3410.782720	17.218535	-0.093840	3.178529
494.553270	3402.820507	17.223539	-0.093766	3.174932
494.935880	3394.741007	17.228544	-0.093832	3.171310
494.596402	3386.769337	17.233549	-0.093763	3.167702
494.600484	3378.769208	17.238554	-0.093759	3.164092
494.214729	3370.890269	17.243559	-0.093682	3.160515
494.310878	3362.828314	17.248563	-0.093695	3.156872
494.477107	3354.834187	17.253568	-0.093720	3.153260
494.276655	3346.812299	17.258573	-0.093678	3.149614
494.024468	3338.901148	17.263578	-0.093626	3.146011
493.999110	3330.868960	17.268583	-0.093616	3.142360
493.887610	3322.897178	17.273587	-0.093590	3.138728
493.891758	3314.908132	17.278592	-0.093585	3.135090
493.852516	3306.905308	17.283597	-0.093573	3.131439
494.097627	3298.858903	17.288602	-0.093613	3.127776
493.810677	3290.894717	17.293607	-0.093554	3.124123
493.491203	3283.001203	17.298611	-0.093490	3.120496
493.998474	3274.934059	17.303616	-0.093579	3.116823
493.488566	3267.002799	17.308621	-0.093479	3.113162
493.793161	3258.952304	17.313626	-0.093530	3.109479
493.456546	3251.015869	17.318631	-0.093462	3.105814
493.688702	3242.973238	17.323635	-0.093500	3.102123
493.385788	3235.049047	17.328640	-0.093438	3.098457
493.080385	3227.087308	17.333645	-0.093376	3.094768
492.755875	3219.165525	17.338650	-0.093311	3.091094
492.778671	3211.132987	17.343655	-0.093310	3.087379
492.714272	3203.102153	17.348659	-0.093292	3.083657
492.942809	3195.120438	17.353664	-0.093330	3.079967
492.994470	3187.104441	17.358669	-0.093334	3.076249
493.006221	3179.113618	17.363674	-0.093331	3.072535
492.986145	3171.114264	17.368679	-0.093322	3.068812
492.410478	3163.183159	17.373683	-0.093210	3.065089
492.650960	3155.201900	17.378688	-0.093249	3.061378
492.804686	3147.126926	17.383693	-0.093273	3.057614
492.789128	3139.184100	17.388698	-0.093264	3.053899
492.962199	3131.166075	17.393703	-0.093291	3.050154
492.532059	3123.243783	17.398707	-0.093206	3.046419
493.015808	3115.235633	17.403712	-0.093291	3.042684
492.827624	3107.256681	17.408717	-0.093251	3.038926
492.824004	3099.286321	17.413722	-0.093245	3.035176
493.156129	3091.229737	17.418727	-0.093301	3.031397
492.511261	3083.354280	17.423731	-0.093176	3.027650
492.584865	3075.341409	17.428736	-0.093185	3.023870
493.119387	3067.243158	17.433741	-0.093279	3.020067
493.130379	3059.334593	17.438746	-0.093276	3.016324
493.134166	3051.328656	17.443751	-0.093271	3.012529
492.629239	3043.441207	17.448755	-0.093172	3.008760
492.457211	3035.472146	17.453760	-0.093135	3.004964
492.102717	3027.539184	17.458765	-0.093063	3.001172
491.918980	3019.562247	17.463770	-0.093024	2.997362
492.181758	3011.498241	17.468775	-0.093068	2.993528
492.221086	3003.487888	17.473779	-0.093070	2.989704
492.215598	2995.512132	17.478784	-0.093063	2.985890
491.893497	2987.545980	17.483789	-0.092998	2.982058
492.654433	2979.445305	17.488794	-0.093135	2.978213
492.203593	2971.538989	17.493799	-0.093045	2.974394
492.406260	2963.508385	17.498803	-0.093078	2.970544
492.304972	2955.598036	17.503808	-0.093054	2.966731
492.381229	2947.575781	17.508813	-0.093063	2.962869
492.387367	2939.616800	17.513818	-0.093059	2.959028
492.530198	2931.630716	17.518823	-0.093080	2.955176
492.061115	2923.711833	17.523827	-0.092988	2.951320
491.871626	2915.746691	17.528832	-0.092947	2.947451
491.747245	2907.742560	17.533837	-0.092919	2.943561
491.826540	2899.765346	17.538842	-0.092928	2.939690
491.926903	2891.771917	17.543847	-0.092942	2.935807
491.917876	2883.744643	17.548851	-0.092935	2.931897
491.774101	2875.802383	17.553856	-0.092903	2.928016
491.978256	2867.735962	17.558861	-0.092935	2.924087
492.058886	2859.811287	17.563866	-0.092945	2.920216
491.861107	2851.879410	17.568871	-0.092903	2.916322
492.274451	2843.776708	17.573875	-0.092975	2.912371
491.740297	2835.871155	17.578880	-0.092870	2.908460
491.578565	2827.864725	17.583885	-0.092835	2.904515
491.329113	2819.950628	17.588890	-0.092783	2.900605
491.403229	2811.941031	17.593895	-0.092792	2.896661
491.434093	2803.923751	17.598899	-0.092792	2.892704
491.650178	2795.921953	17.603904	-0.092827	2.888761
491.258318	2787.990877	17.608909	-0.092749	2.884813
491.048457	2780.082545	17.613914	-0.092705	2.880881
490.795946	2772.128951	17.618919	-0.092653	2.876919
491.108023	2764.051950	17.623923	-0.092705	2.872921
490.974800	2756.103943	17.628928	-0.092675	2.868958
490.763858	2748.100039	17.633933	-0.092631	2.864956
490.434313	2740.209611	17.638938	-0.092564	2.860999
490.410878	2732.211934	17.643943	-0.092555	2.857000
490.581184	2724.160457	17.648947	-0.092581	2.852980
490.539029	2716.166814	17.653952	-0.092568	2.848970
490.187390	2708.211637	17.658957	-0.092497	2.844957
490.233150	2700.264715	17.663962	-0.092501	2.840965
490.197097	2692.294289	17.668967	-0.092489	2.836951
490.458780	2684.243505	17.673971	-0.092532	2.832907
490.234464	2676.333374	17.678976	-0.092485	2.828901
489.675904	2668.379800	17.683981	-0.092376	2.824848
489.645565	2660.408566	17.688986	-0.092365	2.820811
490.364580	2652.294046	17.693991	-0.092494	2.816739
490.849446	2644.236341	17.698995	-0.092579	2.812676
490.299449	2636.396258	17.704000	-0.092471	2.808657
489.728936	2628.474497	17.709005	-0.092360	2.804590
490.036227	2620.477323	17.714010	-0.092412	2.800530
489.919559	2612.529877	17.719015	-0.092385	2.796465
489.406798	2604.590166	17.724019	-0.092284	2.792373
489.343480	2596.609939	17.729024	-0.092267	2.788282
488.990846	2588.609583	17.734029	-0.092196	2.784158
488.760357	2580.681680	17.739034	-0.092148	2.780071
489.035573	2572.641988	17.744039	-0.092194	2.775952
488.878054	2564.659447	17.749043	-0.092159	2.771829
488.976199	2556.670884	17.754048	-0.092172	2.767713
488.987695	2548.663306	17.759053	-0.092169	2.763576
488.744694	2540.747179	17.764058	-0.092119	2.759464
488.637298	2532.800471	17.769063	-0.092094	2.755339
488.464624	2524.761669	17.774067	-0.092056	2.751156
488.548876	2516.760525	17.779072	-0.092067	2.747001
488.078979	2508.834872	17.784077	-0.091974	2.742845
488.268016	2500.820950	17.789082	-0.092004	2.738678
488.350637	2492.821646	17.794087	-0.092014	2.734506
488.450370	2484.828881	17.799091	-0.092027	2.730331
488.016620	2476.919814	17.804096	-0.091941	2.726161
488.182512	2468.887060	17.809101	-0.091967	2.721957
487.753609	2461.045427	17.814106	-0.091882	2.717809
488.074957	2452.984190	17.819111	-0.091937	2.713587
487.852144	2445.048739	17.824115	-0.091890	2.709390
488.163914	2436.999225	17.829120	-0.091943	2.705160
487.788537	2429.074580	17.834125	-0.091868	2.700946
487.810041	2421.096850	17.839130	-0.091866	2.696723
488.064654	2413.075138	17.844135	-0.091908	2.692484
488.016364	2405.082688	17.849139	-0.091894	2.688235
488.029664	2397.143493	17.854144	-0.091892	2.684012
488.240156	2389.137761	17.859149	-0.091925	2.679759
488.087808	2381.249622	17.864154	-0.091892	2.675539
487.859829	2373.278215	17.869159	-0.091844	2.671262
488.142373	2365.210673	17.874163	-0.091892	2.666961
487.698663	2357.347871	17.879168	-0.091804	2.662715
487.460727	2349.391909	17.884173	-0.091754	2.658425
487.073107	2341.477169	17.889178	-0.091677	2.654141
487.128047	2333.452386	17.894183	-0.091682	2.649819
487.321887	2325.413716	17.899187	-0.091713	2.645493
487.467817	2317.455435	17.904192	-0.091735	2.641199
487.242894	2309.479248	17.909197	-0.091688	2.636864
487.525284	2301.470453	17.914202	-0.091735	2.632539
487.199471	2293.561847	17.919207	-0.091669	2.628219
487.003425	2285.598730	17.924211	-0.091627	2.623872
486.931686	2277.659207	17.929216	-0.091609	2.619539
486.572949	2269.725777	17.934221	-0.091537	2.615182
486.519225	2261.728935	17.939226	-0.091521	2.610804
486.497151	2253.731616	17.944231	-0.091512	2.606420
486.767331	2245.693556	17.949235	-0.091557	2.602027
486.597852	2237.804597	17.954240	-0.091520	2.597679
486.382249	2229.830228	17.959245	-0.091475	2.593272
486.603711	2221.714203	17.964250	-0.091511	2.588810
486.382102	2213.779042	17.969255	-0.091464	2.584410
486.017749	2205.878348	17.974259	-0.091391	2.580011
485.959659	2197.946461	17.979264	-0.091375	2.575609
486.002573	2189.914578	17.984269	-0.091378	2.571151
486.117927	2181.919651	17.989274	-0.091394	2.566711
485.885639	2173.996597	17.994279	-0.091346	2.562278
485.679770	2166.085427	17.999283	-0.091302	2.557846
485.868785	2158.063084	18.004288	-0.091332	2.553373
485.839687	2150.066622	18.009293	-0.091322	2.548891
486.094012	2142.067222	18.014298	-0.091364	2.544419
485.963266	2134.160093	18.019303	-0.091334	2.539964
486.006935	2126.167042	18.024307	-0.091337	2.535465
485.953798	2118.242024	18.029312	-0.091322	2.530989
486.008729	2110.249844	18.034317	-0.091327	2.526475
486.272568	2102.242001	18.039322	-0.091371	2.521960
485.830301	2094.401169	18.044327	-0.091283	2.517480
486.078893	2086.363289	18.049331	-0.091324	2.512930
485.612740	2078.475729	18.054336	-0.091232	2.508405
485.773901	2070.432079	18.059341	-0.091257	2.503829
485.661769	2062.506412	18.064346	-0.091231	2.499292
485.407089	2054.588639	18.069351	-0.091178	2.494741
485.521004	2046.540738	18.074355	-0.091194	2.490134
485.834549	2038.553049	18.079360	-0.091248	2.485568
485.596123	2030.647200	18.084365	-0.091198	2.480999
484.936860	2022.797757	18.089370	-0.091070	2.476423
484.969193	2014.809892	18.094375	-0.091071	2.471811
484.979264	2006.805069	18.099379	-0.091067	2.467178
485.288606	1998.775745	18.104384	-0.091120	2.462545
484.962650	1990.862762	18.109389	-0.091054	2.457923
485.054885	1982.886274	18.114394	-0.091066	2.453286
485.174804	1974.889331	18.119399	-0.091083	2.448632
484.868538	1966.949861	18.124403	-0.091021	2.443969
484.737929	1959.063255	18.129408	-0.090991	2.439341
484.706074	1951.075995	18.134413	-0.090980	2.434654
484.692237	1943.075471	18.139418	-0.090972	2.429951
484.923731	1935.042254	18.144423	-0.091010	2.425239
484.450960	1927.174391	18.149427	-0.090917	2.420560
484.328818	1919.248988	18.154432	-0.090889	2.415865
484.094467	1911.271867	18.159437	-0.090840	2.411122
483.972411	1903.321876	18.164442	-0.090812	2.406394
484.122987	1895.323596	18.169447	-0.090835	2.401650
483.783833	1887.424108	18.174451	-0.090767	2.396917
483.535904	1879.508615	18.179456	-0.090715	2.392171
483.649748	1871.481159	18.184461	-0.090731	2.387379
483.347755	1863.563111	18.189466	-0.090670	2.382608
483.349530	1855.578406	18.194471	-0.090665	2.377813
483.548548	1847.557290	18.199475	-0.090697	2.373002
483.516232	1839.611723	18.204480	-0.090685	2.368208
483.414039	1831.660735	18.209485	-0.090661	2.363395
483.172670	1823.772404	18.214490	-0.090611	2.358599
483.392037	1815.760683	18.219495	-0.090647	2.353756
483.062566	1807.834180	18.224499	-0.090580	2.348910
482.713953	1799.942462	18.229504	-0.090510	2.344073
482.879816	1791.918009	18.234509	-0.090536	2.339188
483.302132	1783.871654	18.239514	-0.090609	2.334301
483.317180	1775.941989	18.244519	-0.090607	2.329441
483.257405	1767.997455	18.249523	-0.090590	2.324555
483.337701	1760.063641	18.254528	-0.090600	2.319678
482.779294	1752.201182	18.259533	-0.090491	2.314780
482.718963	1744.251006	18.264538	-0.090474	2.309860
482.738165	1736.272128	18.269543	-0.090473	2.304918
482.398742	1728.359476	18.274547	-0.090404	2.299976
482.263281	1720.422137	18.279552	-0.090374	2.295025
482.312818	1712.414192	18.284557	-0.090378	2.290036
482.379866	1704.448176	18.289562	-0.090385	2.285063
482.122221	1696.554119	18.294567	-0.090332	2.280097
482.077769	1688.573085	18.299571	-0.090318	2.275083
482.267128	1680.557111	18.304576	-0.090348	2.270057
482.178488	1672.581084	18.309581	-0.090327	2.265021
482.363407	1664.621270	18.314586	-0.090356	2.260008
481.759440	1656.796624	18.319591	-0.090238	2.254999
481.497840	1648.850076	18.324595	-0.090184	2.249932
481.477691	1640.886606	18.329600	-0.090175	2.244865
481.310954	1632.962868	18.334605	-0.090139	2.239798
481.830382	1624.895549	18.339610	-0.090231	2.234689
482.011400	1616.942263	18.344615	-0.090259	2.229611
481.788528	1609.023910	18.349619	-0.090212	2.224508
481.702294	1601.123775	18.354624	-0.090191	2.219417
481.852946	1593.118955	18.359629	-0.090214	2.214269
481.289366	1585.297152	18.364634	-0.090104	2.209161
481.727489	1577.240778	18.369639	-0.090180	2.203981
481.230922	1569.404966	18.374643	-0.090083	2.198847
481.117746	1561.462784	18.379648	-0.090056	2.193667
481.240038	1553.461795	18.384653	-0.090074	2.188457
480.968418	1545.563638	18.389658	-0.090018	2.183266
481.081362	1537.583569	18.394663	-0.090034	2.178045
481.018574	1529.631689	18.399667	-0.090017	2.172813
480.886227	1521.717912	18.404672	-0.089987	2.167587
480.597683	1513.789669	18.409677	-0.089928	2.162324
480.331765	1505.909242	18.414682	-0.089874	2.157082
480.765516	1497.874342	18.419687	-0.089949	2.151791
480.833680	1489.903828	18.424691	-0.089956	2.146495
480.263104	1482.090052	18.429696	-0.089845	2.141230
480.609683	1474.050596	18.434701	-0.089904	2.135888
480.851688	1466.083026	18.439706	-0.089944	2.130572
480.342895	1458.222347	18.444711	-0.089844	2.125241
480.400655	1450.275139	18.449715	-0.089850	2.119893
480.326182	1442.383209	18.454720	-0.089831	2.114557
480.337309	1434.361131	18.459725	-0.089828	2.109127
479.865401	1426.500943	18.464730	-0.089735	2.103745
480.321388	1418.475354	18.469735	-0.089814	2.098329
480.326915	1410.526488	18.474739	-0.089810	2.092906
480.746025	1402.527944	18.479744	-0.089883	2.087477
480.247879	1394.693842	18.484749	-0.089785	2.082054
480.475995	1386.742730	18.489754	-0.089822	2.076610
480.240370	1378.859943	18.494759	-0.089773	2.071152
480.283627	1370.894798	18.499763	-0.089776	2.065650
480.244898	1362.999946	18.504768	-0.089764	2.060175
480.401056	1355.023683	18.509773	-0.089787	2.054648
480.123966	1347.146502	18.514778	-0.089731	2.049130
480.095394	1339.224260	18.519783	-0.089720	2.043592
480.354812	1331.251908	18.524787	-0.089763	2.038034
480.402884	1323.348237	18.529792	-0.089767	2.032486
479.954410	1315.484330	18.534797	-0.089678	2.026900
479.801695	1307.566465	18.539802	-0.089645	2.021291
479.359933	1299.701160	18.544807	-0.089557	2.015673
479.014193	1291.796905	18.549811	-0.089488	2.010022
479.739554	1283.710779	18.554816	-0.089617	2.004339
479.543419	1275.832870	18.559821	-0.089576	1.998690
479.065518	1268.008213	18.564826	-0.089482	1.993034
479.086213	1260.051956	18.569831	-0.089480	1.987320
479.045556	1252.109522	18.574835	-0.089468	1.981593
479.142653	1244.180897	18.579840	-0.089480	1.975874
478.803864	1236.281629	18.584845	-0.089412	1.970113
479.126717	1228.314297	18.589850	-0.089467	1.964357
479.217620	1220.403965	18.594855	-0.089479	1.958601
478.510143	1212.601967	18.599859	-0.089342	1.952819
478.625300	1204.633363	18.604864	-0.089358	1.946988
478.304135	1196.743831	18.609869	-0.089293	1.941150
478.065303	1188.849165	18.614874	-0.089244	1.935300
478.162585	1180.882714	18.619879	-0.089256	1.929416
478.776208	1172.834457	18.624883	-0.089365	1.923511
478.486228	1165.002413	18.629888	-0.089306	1.917647
478.220454	1157.110722	18.634893	-0.089252	1.911724
478.387067	1149.156220	18.639898	-0.089277	1.905784
477.954982	1141.340541	18.644903	-0.089192	1.899861
477.834170	1133.424470	18.649907	-0.089164	1.893880
477.963318	1125.485711	18.654912	-0.089183	1.887892
477.504348	1117.641563	18.659917	-0.089092	1.881888
477.274753	1109.772625	18.664922	-0.089044	1.875873
477.673476	1101.760348	18.669927	-0.089113	1.869802
477.468803	1093.866897	18.674931	-0.089070	1.863731
477.512355	1085.966932	18.679936	-0.089073	1.857665
477.028383	1078.125552	18.684941	-0.088978	1.851562
477.057169	1070.192939	18.689946	-0.088978	1.845429
477.198485	1062.265299	18.694951	-0.088999	1.839293
477.446556	1054.316282	18.699955	-0.089040	1.833133
477.966279	1046.329482	18.704960	-0.089132	1.826955
477.034827	1038.611195	18.709965	-0.088953	1.820791
477.231356	1030.672526	18.714970	-0.088984	1.814570
477.151678	1022.800662	18.719975	-0.088964	1.808346
476.957740	1014.923868	18.724979	-0.088923	1.802083
476.468693	1007.140193	18.729984	-0.088827	1.795835
476.943523	999.075408	18.734989	-0.088910	1.789461
476.761652	991.209169	18.739994	-0.088871	1.783141
477.093889	983.255163	18.744999	-0.088928	1.776793
476.695136	975.437247	18.750003	-0.088848	1.770439
476.725282	967.535297	18.755008	-0.088849	1.764049
476.976117	959.620106	18.760013	-0.088890	1.757653
476.904268	951.741894	18.765018	-0.088872	1.751223
477.025148	943.844716	18.770023	-0.088889	1.744778
477.005743	935.983004	18.775027	-0.088880	1.738320
476.641395	928.185762	18.780032	-0.088807	1.731847
476.656726	920.265020	18.785037	-0.088805	1.725296
476.743414	912.406016	18.790042	-0.088816	1.718781
476.559214	904.561444	18.795047	-0.088777	1.712218
476.005157	896.743653	18.800051	-0.088668	1.705603
475.726920	888.924771	18.805056	-0.088611	1.698998
475.714389	881.015212	18.810061	-0.088604	1.692326
475.955512	873.060360	18.815066	-0.088643	1.685623
475.700250	865.248947	18.820071	-0.088591	1.678948
475.557852	857.392638	18.825075	-0.088559	1.672224
475.681093	849.479593	18.830080	-0.088577	1.665460
475.297677	841.680982	18.835085	-0.088500	1.658698
475.443547	833.769729	18.840090	-0.088522	1.651883
475.615310	825.870971	18.845095	-0.088549	1.645054
475.476232	818.038873	18.850099	-0.088518	1.638212
475.187185	810.224568	18.855104	-0.088459	1.631336
474.681589	802.408445	18.860109	-0.088360	1.624399
475.208709	794.448926	18.865114	-0.088453	1.617451
474.228128	786.770126	18.870119	-0.088265	1.610507
474.451957	778.831185	18.875123	-0.088302	1.603474
475.013630	770.879708	18.880128	-0.088401	1.596448
474.798034	763.068006	18.885133	-0.088356	1.589403
474.677488	755.240873	18.890138	-0.088328	1.582328
474.610630	747.403857	18.895143	-0.088311	1.575219
474.564946	739.565070	18.900147	-0.088297	1.568079
474.419412	731.766191	18.905152	-0.088265	1.560929
474.597019	723.889196	18.910157	-0.088293	1.553722
474.463144	716.067776	18.915162	-0.088263	1.546486
474.265623	708.271528	18.920167	-0.088221	1.539229
474.519573	700.379229	18.925171	-0.088263	1.531917
474.534698	692.562450	18.930176	-0.088261	1.524605
473.957209	684.837438	18.935181	-0.088148	1.517253
473.831779	677.028060	18.940186	-0.088119	1.509854
474.159744	669.142097	18.945191	-0.088175	1.502417
473.822645	661.374117	18.950195	-0.088107	1.494952
473.882509	653.544190	18.955200	-0.088113	1.487452
473.560152	645.785722	18.960205	-0.088048	1.479922
473.198986	638.037399	18.965210	-0.087976	1.472358
473.143048	630.179151	18.970215	-0.087960	1.464696
473.263468	622.338851	18.975219	-0.087978	1.457039
473.260523	614.534670	18.980224	-0.087972	1.449358
472.657604	606.829782	18.985229	-0.087855	1.441637
472.820970	598.994767	18.990234	-0.087880	1.433870
472.967575	591.157958	18.995239	-0.087902	1.426056
472.241925	583.503022	19.000243	-0.087762	1.418237
472.354002	575.665981	19.005248	-0.087778	1.410330
472.266524	567.881988	19.010253	-0.087756	1.402399
472.469705	560.078536	19.015258	-0.087789	1.394453
471.874364	552.394251	19.020263	-0.087673	1.386447
472.103772	544.552921	19.025267	-0.087711	1.378374
472.080664	536.790930	19.030272	-0.087701	1.370292
472.030311	529.013755	19.035277	-0.087687	1.362142
472.096298	521.246043	19.040282	-0.087694	1.353972
471.765724	513.544706	19.045287	-0.087627	1.345754
471.797620	505.771457	19.050291	-0.087628	1.337473
472.118344	497.963455	19.055296	-0.087683	1.329155
471.661510	490.317274	19.060301	-0.087593	1.320818
471.320414	482.613267	19.065306	-0.087524	1.312387
470.969587	474.860197	19.070311	-0.087454	1.303845
471.270939	467.047743	19.075315	-0.087505	1.295303
471.303449	459.323568	19.080320	-0.087506	1.286751
470.950057	451.674664	19.085325	-0.087435	1.278154
470.719505	443.989221	19.090330	-0.087387	1.269481
470.654643	436.285529	19.095335	-0.087370	1.260759
470.266615	428.651898	19.100339	-0.087293	1.251994
470.609280	420.862259	19.105344	-0.087351	1.243129
470.491095	413.198730	19.110349	-0.087324	1.234257
470.354531	405.516716	19.115354	-0.087294	1.225295
470.467305	397.809905	19.120359	-0.087310	1.216288
469.754621	390.252745	19.125363	-0.087172	1.207225
470.009263	382.537385	19.130368	-0.087214	1.198100
470.045503	374.855241	19.135373	-0.087216	1.188901
469.988725	367.207069	19.140378	-0.087201	1.179652
470.171312	359.524182	19.145383	-0.087230	1.170337
469.902431	351.936310	19.150387	-0.087175	1.160970
469.725931	344.332114	19.155392	-0.087137	1.151525
469.575215	336.696197	19.160397	-0.087104	1.141969
469.876048	329.017033	19.165402	-0.087155	1.132374
469.630180	321.456298	19.170407	-0.087104	1.122729
469.390431	313.898486	19.175411	-0.087054	1.113006
469.486260	306.287321	19.180416	-0.087067	1.103202
469.256552	298.750098	19.185421	-0.087019	1.093334
469.362313	291.145598	19.190426	-0.087034	1.083364
468.971075	283.665437	19.195431	-0.086956	1.073352
469.022950	276.082512	19.200435	-0.086961	1.063211
469.099458	268.527397	19.205440	-0.086970	1.053015
468.801383	261.046744	19.210445	-0.086910	1.042733
468.726815	253.541295	19.215450	-0.086891	1.032368
468.606604	246.052563	19.220455	-0.086864	1.021910
468.292641	238.605208	19.225459	-0.086800	1.011354
468.390461	231.099014	19.230464	-0.086814	1.000705
468.116908	223.663239	19.235469	-0.086758	0.989950
467.659846	216.262113	19.240474	-0.086668	0.979081
467.718775	208.789287	19.245479	-0.086674	0.968117
467.732168	201.347348	19.250483	-0.086672	0.957061
468.068214	193.862267	19.255488	-0.086729	0.945896
467.600714	186.554021	19.260493	-0.086637	0.934653
467.432570	179.197003	19.265498	-0.086601	0.923279
467.584610	171.813370	19.270503	-0.086625	0.911809
466.975059	164.566365	19.275507	-0.086506	0.900198
466.783165	157.273067	19.280512	-0.086466	0.888478
466.664868	149.970834	19.285517	-0.086439	0.876608
466.716863	142.667983	19.290522	-0.086444	0.864623
466.486733	135.445685	19.295527	-0.086396	0.852522
466.074154	128.269513	19.300531	-0.086315	0.840270
465.852360	121.076088	19.305536	-0.086269	0.827865
465.806146	113.867757	19.310541	-0.086256	0.815300
465.593939	106.719596	19.315546	-0.086211	0.802592
466.037584	99.495864	19.320551	-0.086289	0.789754
465.820776	92.419506	19.325555	-0.086244	0.776759
465.418290	85.413614	19.330560	-0.086165	0.763613
465.238952	78.395502	19.335565	-0.086127	0.750289
465.007911	71.598493	19.340570	-0.086079	0.737136