Mon Apr 19 09:52:54 2021

Number of Points = 3639
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.502287	-0.150286	0.000000	-0.000145	0.310202

1.572243	0.023241	0.005005	0.000028	0.310223
2.198088	-0.094207	0.010010	-0.000088	0.310206
2.144245	-0.081050	0.015014	-0.000078	0.310221
2.434085	-0.139146	0.020019	-0.000132	0.310196
1.491336	0.039593	0.025024	0.000043	0.310231
1.385943	0.059756	0.030029	0.000063	0.310236
1.086991	0.117194	0.035034	0.000118	0.310250
1.223606	0.092229	0.040038	0.000093	0.310250
1.353305	0.065202	0.045043	0.000069	0.310233
1.322741	0.076084	0.050048	0.000075	0.310258
1.007350	0.122061	0.055053	0.000133	0.310205
1.268788	0.014164	0.060058	0.000085	0.309924
1.373566	-0.003504	0.065062	0.000065	0.309930
1.695403	-0.067580	0.070067	0.000005	0.309904
1.647705	-0.054866	0.075072	0.000014	0.309923
1.526067	-0.034319	0.080077	0.000037	0.309916
2.083270	-0.139698	0.085082	-0.000067	0.309896
2.044032	-0.131932	0.090086	-0.000060	0.309899
1.688918	-0.076785	0.095091	0.000007	0.309855
1.636275	-0.123852	0.100096	0.000016	0.309591
1.899576	-0.176059	0.105101	-0.000033	0.309570
2.282249	-0.249045	0.110106	-0.000104	0.309554
2.429936	-0.274861	0.115110	-0.000131	0.309559
1.703518	-0.147976	0.120115	0.000004	0.309535
1.664867	-0.191891	0.125120	0.000011	0.309297
1.508202	-0.163838	0.130125	0.000040	0.309295
1.665973	-0.191078	0.135130	0.000011	0.309302
1.732971	-0.204225	0.140134	-0.000002	0.309297
1.823712	-0.259038	0.145139	-0.000018	0.309118
1.960398	-0.319372	0.150144	-0.000044	0.308952
1.931129	-0.315456	0.155149	-0.000038	0.308945
2.447377	-0.413459	0.160154	-0.000135	0.308926
2.608900	-0.500293	0.165158	-0.000165	0.308656
2.066825	-0.406712	0.170163	-0.000064	0.308633
1.983272	-0.389481	0.175168	-0.000048	0.308643
2.143775	-0.471057	0.180173	-0.000078	0.308397
1.921994	-0.448404	0.185178	-0.000037	0.308314
1.817373	-0.427975	0.190182	-0.000017	0.308321
2.064459	-0.516605	0.195187	-0.000063	0.308116
2.038383	-0.530500	0.200192	-0.000058	0.308028
1.966359	-0.519235	0.205197	-0.000045	0.308020
2.151190	-0.611077	0.210202	-0.000079	0.307746
2.048323	-0.605383	0.215206	-0.000060	0.307685
2.340469	-0.672782	0.220211	-0.000114	0.307617
1.900128	-0.642802	0.225216	-0.000033	0.307382
2.080584	-0.680381	0.230221	-0.000066	0.307360
1.304326	-0.572848	0.235226	0.000078	0.307202
1.801658	-0.692860	0.240230	-0.000014	0.307062
1.639930	-0.668558	0.245235	0.000016	0.307038
1.138882	-0.629110	0.250240	0.000109	0.306795
1.409795	-0.681991	0.255245	0.000059	0.306778
1.258742	-0.687149	0.260250	0.000087	0.306624
1.040993	-0.682726	0.265254	0.000127	0.306458
1.625081	-0.799009	0.270259	0.000019	0.306410
1.748403	-0.882777	0.275264	-0.000004	0.306120
1.345778	-0.808811	0.280269	0.000071	0.306124
1.919580	-0.969146	0.285274	-0.000036	0.305859
2.231555	-1.041336	0.290278	-0.000094	0.305786
2.026584	-1.046240	0.295283	-0.000056	0.305586
2.200794	-1.089984	0.300288	-0.000088	0.305529
2.116067	-1.135814	0.305293	-0.000072	0.305239
2.073568	-1.139612	0.310298	-0.000065	0.305184
2.119512	-1.211847	0.315302	-0.000073	0.304881
1.859803	-1.174373	0.320307	-0.000025	0.304835
2.082119	-1.276288	0.325312	-0.000066	0.304543
1.313043	-1.149176	0.330317	0.000077	0.304483
1.607721	-1.249558	0.335322	0.000022	0.304260
1.449086	-1.246272	0.340326	0.000052	0.304139
1.305726	-1.265692	0.345331	0.000079	0.303923
1.279465	-1.294139	0.350336	0.000083	0.303764
1.956854	-1.450560	0.355341	-0.000043	0.303606
1.847518	-1.486500	0.360346	-0.000022	0.303340
2.297222	-1.593597	0.365350	-0.000106	0.303219
2.123117	-1.610779	0.370355	-0.000073	0.302986
2.356293	-1.697687	0.375360	-0.000117	0.302773
2.370613	-1.737366	0.380365	-0.000119	0.302596
2.131124	-1.750854	0.385370	-0.000075	0.302323
2.291132	-1.818474	0.390374	-0.000105	0.302138
1.995886	-1.800076	0.395379	-0.000050	0.301970
2.151455	-1.880929	0.400384	-0.000079	0.301718
1.478120	-1.800466	0.405389	0.000047	0.301517
2.079259	-1.947754	0.410394	-0.000065	0.301334
1.645784	-1.919866	0.415398	0.000016	0.301090
1.481303	-1.937972	0.420403	0.000046	0.300859
2.178035	-2.098402	0.425408	-0.000083	0.300696
2.268456	-2.151593	0.430413	-0.000100	0.300519
1.895625	-2.150613	0.435418	-0.000031	0.300198
1.504799	-2.116631	0.440422	0.000042	0.300019
1.358268	-2.128475	0.445427	0.000069	0.299834
1.472429	-2.209058	0.450432	0.000048	0.299545
0.853180	-2.137804	0.455437	0.000163	0.299345
1.412412	-2.280133	0.460442	0.000059	0.299148
1.324227	-2.309363	0.465446	0.000076	0.298929
0.874286	-2.290942	0.470451	0.000159	0.298623
1.447465	-2.436028	0.475456	0.000053	0.298424
1.942380	-2.574871	0.480461	-0.000039	0.298187
1.195187	-2.476359	0.485466	0.000100	0.298006
1.084133	-2.524660	0.490470	0.000121	0.297674
1.203027	-2.593520	0.495475	0.000098	0.297444
0.896290	-2.583470	0.500480	0.000156	0.297222
-0.088707	-2.446967	0.505485	0.000339	0.297014
-0.976522	-2.341916	0.510490	0.000504	0.296740
-1.220849	-2.328173	0.515494	0.000550	0.296591
-1.351151	-2.339372	0.520499	0.000574	0.296420
-1.029652	-2.458725	0.525504	0.000514	0.296123
-1.190535	-2.468019	0.530509	0.000544	0.295934
-1.588022	-2.430346	0.535514	0.000618	0.295765
-1.242545	-2.540168	0.540518	0.000554	0.295535
-1.301403	-2.572587	0.545523	0.000565	0.295324
-2.157277	-2.448605	0.550528	0.000724	0.295169
-2.701997	-2.407490	0.555533	0.000825	0.294885
-2.401824	-2.496590	0.560538	0.000770	0.294716
-2.824510	-2.452579	0.565542	0.000848	0.294555
-3.205089	-2.440319	0.570547	0.000919	0.294275
-3.134659	-2.476115	0.575552	0.000906	0.294162
-3.498360	-2.458193	0.580557	0.000974	0.293925
-3.698282	-2.466624	0.585562	0.001011	0.293704
-3.782009	-2.470676	0.590566	0.001027	0.293609
-4.122812	-2.473497	0.595571	0.001090	0.293290
-3.712971	-2.570728	0.600576	0.001014	0.293178
-4.274868	-2.506026	0.605581	0.001118	0.292993
-4.269899	-2.559392	0.610586	0.001117	0.292734
-4.578179	-2.524006	0.615590	0.001175	0.292632
-5.331518	-2.445227	0.620595	0.001315	0.292344
-5.024972	-2.521458	0.625600	0.001258	0.292243
-6.084410	-2.366472	0.630605	0.001455	0.292056
-6.561930	-2.307395	0.635610	0.001544	0.291919
-7.020242	-2.251162	0.640614	0.001629	0.291785
-6.759229	-2.330977	0.645619	0.001581	0.291624
-6.926370	-2.339359	0.650624	0.001612	0.291432
-6.935495	-2.366723	0.655629	0.001614	0.291288
-7.094389	-2.373482	0.660634	0.001643	0.291110
-7.267365	-2.366914	0.665638	0.001675	0.290987
-7.740807	-2.320111	0.670643	0.001764	0.290792
-7.463347	-2.390865	0.675648	0.001712	0.290690
-7.001591	-2.507604	0.680653	0.001626	0.290527
-7.979829	-2.365268	0.685658	0.001808	0.290350
-8.141536	-2.365561	0.690662	0.001838	0.290202
-8.359350	-2.357333	0.695667	0.001879	0.290046
-8.777781	-2.311017	0.700672	0.001957	0.289897
-8.781348	-2.335475	0.705677	0.001957	0.289772
-8.812768	-2.373871	0.710682	0.001963	0.289552
-8.636263	-2.420340	0.715686	0.001930	0.289480
-9.003380	-2.399522	0.720691	0.001999	0.289250
-8.657793	-2.479002	0.725696	0.001934	0.289167
-9.212785	-2.426314	0.730701	0.002038	0.288925
-9.347671	-2.415405	0.735706	0.002063	0.288857
-9.714347	-2.395209	0.740710	0.002131	0.288624
-9.634274	-2.418519	0.745715	0.002116	0.288581
-9.888319	-2.429416	0.750720	0.002163	0.288294
-10.129239	-2.385936	0.755725	0.002208	0.288293
-10.196141	-2.429103	0.760730	0.002221	0.288015
-9.944493	-2.477541	0.765734	0.002174	0.288001
-11.023903	-2.338666	0.770739	0.002375	0.287713
-11.284631	-2.296482	0.775744	0.002423	0.287687
-11.057854	-2.372094	0.780749	0.002381	0.287514
-11.312270	-2.359353	0.785754	0.002429	0.287345
-11.132208	-2.409854	0.790758	0.002395	0.287255
-11.009401	-2.481285	0.795763	0.002372	0.287008
-10.745812	-2.541109	0.800768	0.002323	0.286948
-11.539088	-2.440551	0.805773	0.002471	0.286728
-11.759285	-2.402597	0.810778	0.002512	0.286717
-11.629901	-2.489242	0.815782	0.002488	0.286398
-11.849456	-2.451464	0.820787	0.002529	0.286388
-11.708731	-2.527998	0.825792	0.002502	0.286130
-12.138835	-2.456808	0.830797	0.002582	0.286095
-12.706907	-2.398087	0.835802	0.002688	0.285869
-12.805687	-2.398065	0.840806	0.002707	0.285778
-12.624079	-2.452340	0.845811	0.002673	0.285671
-12.564568	-2.493418	0.850816	0.002662	0.285517
-12.457233	-2.530592	0.855821	0.002642	0.285428
-12.933505	-2.496657	0.860826	0.002730	0.285161
-12.786206	-2.524085	0.865830	0.002703	0.285157
-13.390497	-2.474939	0.870835	0.002816	0.284849
-13.427419	-2.466569	0.875840	0.002822	0.284857
-13.564575	-2.493985	0.880845	0.002848	0.284591
-13.276416	-2.563805	0.885850	0.002794	0.284503
-13.695341	-2.520274	0.890854	0.002872	0.284337
-13.620183	-2.557518	0.895859	0.002858	0.284217
-13.479630	-2.614861	0.900864	0.002832	0.284055
-14.152068	-2.524912	0.905869	0.002957	0.283890
-14.239728	-2.528320	0.910874	0.002974	0.283791
-14.163516	-2.582573	0.915878	0.002960	0.283585
-14.428724	-2.542186	0.920883	0.003009	0.283545
-14.391252	-2.607853	0.925888	0.003002	0.283245
-14.426019	-2.599384	0.930893	0.003008	0.283256
-14.990704	-2.550544	0.935898	0.003113	0.282981
-15.144635	-2.524962	0.940902	0.003142	0.282968
-15.327910	-2.536286	0.945907	0.003176	0.282740
-15.453985	-2.533556	0.950912	0.003200	0.282636
-15.716452	-2.509024	0.955917	0.003249	0.282518
-15.940282	-2.507293	0.960922	0.003290	0.282318
-15.384482	-2.614379	0.965926	0.003187	0.282287
-16.408692	-2.485013	0.970931	0.003377	0.281995
-16.348945	-2.494635	0.975936	0.003366	0.282002
-16.446469	-2.514471	0.980941	0.003385	0.281809
-16.483018	-2.528558	0.985946	0.003391	0.281702
-16.793406	-2.491674	0.990950	0.003449	0.281602
-17.255813	-2.451833	0.995955	0.003535	0.281374
-16.606508	-2.569023	1.000960	0.003414	0.281379
-16.877236	-2.577903	1.005965	0.003465	0.281080
-17.346001	-2.497399	1.010970	0.003552	0.281055
-17.439767	-2.507715	1.015974	0.003569	0.280915
-18.314734	-2.377611	1.020979	0.003732	0.280765
-18.272241	-2.384462	1.025984	0.003724	0.280770
-17.753349	-2.522919	1.030989	0.003628	0.280542
-17.612177	-2.555069	1.035994	0.003602	0.280509
-17.558498	-2.603040	1.040998	0.003592	0.280312
-18.214968	-2.511173	1.046003	0.003714	0.280169
-18.216723	-2.522140	1.051008	0.003714	0.280111
-18.843680	-2.456783	1.056013	0.003831	0.279860
-19.128316	-2.404799	1.061018	0.003884	0.279861
-18.420084	-2.574328	1.066022	0.003752	0.279650
-18.974602	-2.496109	1.071027	0.003855	0.279533
-19.276689	-2.452662	1.076032	0.003911	0.279474
-19.317962	-2.486666	1.081037	0.003919	0.279258
-19.278354	-2.494517	1.086042	0.003912	0.279255
-19.435125	-2.512628	1.091046	0.003941	0.279013
-20.440683	-2.347581	1.096051	0.004128	0.278921
-20.016897	-2.426308	1.101056	0.004049	0.278912
-20.364987	-2.418564	1.106061	0.004114	0.278624
-21.030827	-2.295647	1.111066	0.004238	0.278634
-20.518256	-2.403961	1.116070	0.004143	0.278555
-20.753358	-2.411668	1.121075	0.004186	0.278293
-20.992703	-2.367142	1.126080	0.004231	0.278298
-20.848944	-2.423729	1.131085	0.004204	0.278140
-20.610662	-2.496735	1.136090	0.004160	0.277985
-20.884579	-2.443671	1.141094	0.004211	0.278002
-21.254502	-2.442548	1.146099	0.004280	0.277657
-21.006605	-2.485960	1.151104	0.004234	0.277666
-20.703061	-2.572518	1.156109	0.004177	0.277503
-21.883735	-2.390641	1.161114	0.004397	0.277331
-21.177191	-2.517689	1.166118	0.004265	0.277339
-21.576729	-2.504207	1.171123	0.004340	0.277030
-22.416195	-2.350525	1.176128	0.004496	0.277035
-22.407756	-2.366097	1.181133	0.004494	0.276962
-22.509481	-2.388943	1.186138	0.004513	0.276746
-22.359506	-2.415431	1.191142	0.004485	0.276750
-23.033482	-2.322176	1.196147	0.004611	0.276596
-22.703576	-2.416317	1.201152	0.004549	0.276418
-21.967153	-2.554846	1.206157	0.004412	0.276393
-22.311268	-2.546869	1.211162	0.004476	0.276107
-22.722284	-2.474361	1.216166	0.004553	0.276096
-22.581412	-2.529368	1.221171	0.004527	0.275942
-23.129718	-2.461350	1.226176	0.004629	0.275775
-23.396617	-2.411091	1.231181	0.004678	0.275784
-23.262146	-2.476724	1.236186	0.004653	0.275568
-23.186739	-2.495468	1.241190	0.004639	0.275542
-24.206535	-2.328814	1.246195	0.004829	0.275443
-24.154043	-2.381772	1.251200	0.004819	0.275215
-23.568572	-2.492733	1.256205	0.004711	0.275191
-24.606459	-2.338881	1.261210	0.004904	0.275007
-24.635134	-2.355059	1.266214	0.004909	0.274895
-24.277437	-2.421410	1.271219	0.004842	0.274888
-24.225096	-2.483589	1.276224	0.004833	0.274610
-24.706695	-2.407944	1.281229	0.004922	0.274548
-24.388372	-2.482429	1.286234	0.004863	0.274460
-24.638187	-2.474560	1.291238	0.004910	0.274262
-24.765626	-2.454192	1.296243	0.004933	0.274247
-24.541564	-2.540235	1.301248	0.004892	0.274008
-24.331381	-2.597757	1.306253	0.004853	0.273906
-24.831794	-2.528638	1.311258	0.004946	0.273790
-25.886942	-2.368080	1.316262	0.005142	0.273624
-25.602382	-2.422012	1.321267	0.005089	0.273613
-25.456390	-2.493395	1.326272	0.005062	0.273376
-25.915644	-2.424542	1.331277	0.005147	0.273298
-25.684179	-2.477205	1.336282	0.005104	0.273242
-26.028489	-2.456809	1.341286	0.005168	0.273018
-26.352639	-2.400862	1.346291	0.005229	0.273002
-26.344026	-2.434123	1.351296	0.005227	0.272834
-26.703154	-2.397790	1.356301	0.005294	0.272680
-26.952209	-2.354387	1.361306	0.005340	0.272670
-26.711240	-2.442832	1.366310	0.005296	0.272433
-27.112729	-2.384582	1.371315	0.005370	0.272355
-26.825064	-2.444403	1.376320	0.005317	0.272315
-27.425066	-2.387291	1.381325	0.005428	0.272038
-27.717367	-2.332791	1.386330	0.005483	0.272045
-27.696118	-2.351677	1.391334	0.005479	0.271965
-28.436108	-2.254579	1.396339	0.005617	0.271766
-28.067416	-2.322240	1.401344	0.005548	0.271763
-27.682284	-2.416387	1.406349	0.005476	0.271634
-27.899642	-2.420601	1.411354	0.005517	0.271401
-28.009255	-2.397997	1.416358	0.005537	0.271415
-28.068240	-2.433259	1.421363	0.005548	0.271170
-28.454879	-2.373901	1.426368	0.005620	0.271111
-28.105409	-2.447571	1.431373	0.005555	0.271057
-28.837336	-2.363611	1.436378	0.005691	0.270794
-28.710477	-2.383722	1.441382	0.005668	0.270810
-28.980148	-2.355758	1.446387	0.005718	0.270698
-29.148277	-2.354882	1.451392	0.005749	0.270539
-29.103831	-2.360464	1.456397	0.005741	0.270552
-29.119219	-2.404064	1.461402	0.005744	0.270304
-29.308019	-2.389985	1.466406	0.005779	0.270195
-29.567986	-2.342618	1.471411	0.005827	0.270196
-29.466315	-2.419367	1.476416	0.005809	0.269883
-29.880764	-2.344710	1.481421	0.005886	0.269879
-30.274743	-2.284126	1.486426	0.005959	0.269820
-29.294408	-2.513806	1.491430	0.005777	0.269544
-30.336791	-2.321499	1.496435	0.005971	0.269559
-29.788280	-2.456703	1.501440	0.005868	0.269368
-30.128719	-2.413694	1.506445	0.005932	0.269267
-30.224746	-2.401090	1.511450	0.005950	0.269241
-30.503532	-2.409268	1.516454	0.006002	0.268924
-30.719358	-2.370385	1.521459	0.006042	0.268922
-30.214676	-2.488889	1.526464	0.005948	0.268778
-31.029939	-2.369584	1.531469	0.006100	0.268622
-30.770822	-2.420447	1.536474	0.006051	0.268602
-31.178655	-2.392859	1.541478	0.006127	0.268350
-31.976276	-2.254074	1.546483	0.006276	0.268316
-31.345154	-2.376537	1.551488	0.006158	0.268275
-30.945480	-2.500956	1.556493	0.006084	0.267996
-31.363784	-2.425246	1.561498	0.006162	0.267994
-31.677268	-2.402140	1.566502	0.006220	0.267810
-32.086032	-2.353626	1.571507	0.006296	0.267671
-31.593528	-2.445359	1.576512	0.006205	0.267659
-32.188737	-2.393720	1.581517	0.006315	0.267353
-32.315695	-2.372600	1.586522	0.006339	0.267342
-32.168414	-2.415391	1.591526	0.006312	0.267255
-32.376469	-2.422137	1.596531	0.006350	0.267014
-32.454736	-2.407018	1.601536	0.006365	0.267018
-32.387067	-2.460586	1.606541	0.006352	0.266795
-32.602998	-2.432726	1.611546	0.006393	0.266733
-32.626068	-2.444815	1.616550	0.006397	0.266644
-32.995098	-2.423570	1.621555	0.006466	0.266395
-32.537649	-2.507314	1.626560	0.006380	0.266392
-32.697162	-2.526227	1.631565	0.006410	0.266131
-33.037700	-2.475797	1.636570	0.006473	0.266069
-33.082115	-2.487830	1.641574	0.006482	0.265959
-33.836678	-2.384768	1.646579	0.006622	0.265773
-34.116640	-2.330251	1.651584	0.006674	0.265793
-34.079650	-2.372239	1.656589	0.006667	0.265601
-34.160408	-2.371386	1.661594	0.006682	0.265525
-34.168774	-2.378009	1.666598	0.006684	0.265481
-34.709815	-2.334671	1.671603	0.006785	0.265180
-34.137385	-2.439787	1.676608	0.006678	0.265175
-34.417494	-2.416118	1.681613	0.006730	0.265026
-34.923483	-2.355715	1.686618	0.006825	0.264853
-34.622462	-2.406379	1.691622	0.006769	0.264875
-34.987251	-2.395594	1.696627	0.006836	0.264571
-35.735104	-2.263673	1.701632	0.006976	0.264549
-35.585847	-2.296482	1.706637	0.006948	0.264518
-36.002625	-2.265784	1.711642	0.007025	0.264271
-35.366541	-2.383575	1.716646	0.006907	0.264259
-35.496072	-2.386923	1.721651	0.006931	0.264112
-35.548608	-2.414196	1.726656	0.006941	0.263910
-35.598246	-2.404866	1.731661	0.006950	0.263911
-35.515843	-2.472668	1.736666	0.006935	0.263621
-35.156924	-2.545821	1.741670	0.006868	0.263578
-35.913090	-2.434017	1.746675	0.007009	0.263437
-37.045978	-2.253740	1.751680	0.007220	0.263295
-36.332537	-2.384878	1.756685	0.007087	0.263287
-36.307860	-2.432648	1.761690	0.007082	0.263049
-36.750755	-2.361277	1.766694	0.007165	0.262999
-36.786247	-2.370405	1.771699	0.007171	0.262913
-37.161479	-2.347765	1.776704	0.007241	0.262662
-36.835488	-2.408615	1.781709	0.007181	0.262653
-37.270125	-2.366880	1.786714	0.007261	0.262447
-37.421059	-2.357556	1.791718	0.007290	0.262347
-37.039275	-2.430880	1.796723	0.007218	0.262326
-37.685273	-2.368820	1.801728	0.007339	0.262019
-37.818484	-2.344317	1.806733	0.007364	0.262021
-37.845211	-2.359449	1.811738	0.007368	0.261910
-37.900155	-2.379788	1.816742	0.007379	0.261743
-38.591919	-2.254809	1.821747	0.007507	0.261738
-38.037752	-2.398531	1.826752	0.007404	0.261500
-38.527065	-2.325172	1.831757	0.007495	0.261414
-38.823810	-2.273385	1.836762	0.007551	0.261401
-38.922431	-2.305576	1.841766	0.007569	0.261124
-38.572501	-2.376150	1.846771	0.007504	0.261085
-39.213634	-2.276105	1.851776	0.007623	0.260993
-39.466875	-2.268085	1.856781	0.007670	0.260782
-39.019182	-2.350679	1.861786	0.007587	0.260776
-38.495435	-2.474791	1.866790	0.007490	0.260615
-39.346776	-2.337657	1.871795	0.007648	0.260517
-39.027766	-2.404609	1.876800	0.007589	0.260467
-39.257202	-2.412299	1.881805	0.007631	0.260192
-39.995258	-2.278279	1.886810	0.007769	0.260191
-40.432114	-2.223981	1.891814	0.007850	0.260051
-40.324811	-2.272505	1.896819	0.007830	0.259889
-40.346755	-2.267370	1.901824	0.007834	0.259896
-40.361363	-2.309405	1.906829	0.007837	0.259646
-40.693854	-2.265567	1.911834	0.007899	0.259554
-40.079788	-2.384189	1.916838	0.007785	0.259515
-40.770147	-2.304937	1.921843	0.007913	0.259256
-40.591208	-2.337744	1.926848	0.007880	0.259255
-40.672118	-2.349439	1.931853	0.007895	0.259107
-40.881465	-2.346524	1.936858	0.007934	0.258911
-41.193072	-2.285008	1.941862	0.007992	0.258938
-41.338424	-2.307967	1.946867	0.008019	0.258661
-41.789576	-2.230864	1.951872	0.008103	0.258633
-41.587027	-2.279053	1.956877	0.008065	0.258570
-41.934899	-2.263582	1.961882	0.008130	0.258302
-41.434761	-2.353443	1.966886	0.008037	0.258308
-41.707198	-2.333410	1.971891	0.008088	0.258143
-42.010067	-2.301940	1.976896	0.008144	0.258010
-41.504893	-2.395636	1.981901	0.008050	0.258000
-42.210257	-2.328653	1.986906	0.008181	0.257655
-42.142065	-2.339073	1.991910	0.008168	0.257667
-42.715832	-2.253152	1.996915	0.008275	0.257563
-42.147425	-2.396402	2.001920	0.008170	0.257339

-42.450894	-2.394026	2.011917	0.008226	0.257041
-43.171720	-2.286216	2.021914	0.008360	0.256910
-43.045754	-2.340023	2.031910	0.008337	0.256736
-43.389121	-2.313427	2.041907	0.008401	0.256533
-43.270153	-2.359286	2.051904	0.008379	0.256396
-43.463438	-2.346683	2.061901	0.008414	0.256269
-43.785948	-2.319059	2.071898	0.008475	0.256093
-43.790476	-2.317428	2.081894	0.008475	0.256098
-43.537044	-2.389667	2.091891	0.008428	0.255950
-43.793293	-2.374943	2.101888	0.008476	0.255770
-43.736652	-2.387205	2.111885	0.008465	0.255759
-43.692137	-2.395630	2.121882	0.008457	0.255757
-43.773482	-2.379861	2.131878	0.008472	0.255762
-44.167975	-2.304607	2.141875	0.008546	0.255782
-44.119355	-2.350238	2.151872	0.008537	0.255574
-44.345026	-2.316195	2.161869	0.008579	0.255534
-44.561099	-2.232715	2.171866	0.008619	0.255784
-44.161606	-2.305479	2.181862	0.008544	0.255784
-44.206593	-2.299140	2.191859	0.008553	0.255773
-43.803100	-2.373529	2.201856	0.008478	0.255768
-44.493685	-2.244041	2.211853	0.008606	0.255790
-43.905150	-2.354605	2.221850	0.008497	0.255770
-44.006187	-2.335568	2.231846	0.008515	0.255774
-44.070807	-2.281169	2.241843	0.008527	0.256015
-43.399195	-2.390154	2.251840	0.008402	0.256090
-43.215506	-2.425123	2.261837	0.008368	0.256081
-43.787079	-2.319422	2.271834	0.008475	0.256091
-42.949485	-2.437602	2.281830	0.008319	0.256284
-43.137729	-2.385041	2.291827	0.008354	0.256388
-42.965178	-2.415384	2.301824	0.008322	0.256393
-43.043352	-2.385689	2.311821	0.008336	0.256481
-42.877469	-2.371443	2.321818	0.008305	0.256732
-42.768425	-2.392720	2.331814	0.008285	0.256724
-42.691081	-2.376574	2.341811	0.008271	0.256894
-42.327281	-2.421893	2.351808	0.008203	0.257012
-42.643525	-2.357638	2.361805	0.008262	0.257050
-42.371952	-2.355287	2.371802	0.008211	0.257341
-42.498804	-2.329758	2.381798	0.008235	0.257355
-42.341040	-2.304207	2.391795	0.008205	0.257660
-41.953861	-2.369844	2.401792	0.008133	0.257687
-41.831565	-2.336122	2.411789	0.008110	0.258002
-41.630649	-2.367205	2.421786	0.008073	0.258032
-41.553958	-2.336896	2.431782	0.008059	0.258281
-41.235441	-2.378298	2.441779	0.007999	0.258373
-41.094840	-2.361769	2.451776	0.007973	0.258609
-41.082230	-2.338297	2.461773	0.007971	0.258754
-40.484053	-2.419500	2.471770	0.007860	0.258908
-40.451390	-2.384399	2.481766	0.007853	0.259138
-40.590971	-2.336380	2.491763	0.007879	0.259264
-39.870056	-2.419088	2.501760	0.007745	0.259535
-40.215889	-2.336506	2.511757	0.007810	0.259644
-39.555284	-2.418309	2.521754	0.007687	0.259858
-39.676968	-2.360970	2.531750	0.007709	0.260055
-39.396771	-2.387012	2.541747	0.007657	0.260193
-39.445794	-2.316233	2.551744	0.007666	0.260537
-39.598401	-2.265634	2.561741	0.007695	0.260664
-38.908994	-2.370025	2.571738	0.007566	0.260781
-39.164857	-2.266909	2.581734	0.007614	0.261095
-38.998361	-2.257358	2.591731	0.007583	0.261316
-38.757019	-2.260934	2.601728	0.007538	0.261540
-38.616338	-2.248917	2.611725	0.007512	0.261748
-38.402909	-2.236697	2.621722	0.007472	0.262030
-38.255651	-2.224405	2.631718	0.007444	0.262246
-37.518300	-2.322756	2.641715	0.007307	0.262443
-37.423317	-2.300406	2.651712	0.007290	0.262662
-36.368029	-2.439927	2.661709	0.007093	0.262951
-36.419964	-2.406546	2.671706	0.007103	0.263083
-36.562404	-2.345573	2.681702	0.007129	0.263276
-36.004046	-2.393357	2.691699	0.007025	0.263572
-35.995602	-2.365772	2.701696	0.007024	0.263732
-35.326621	-2.457487	2.711693	0.006899	0.263896
-35.234198	-2.417731	2.721690	0.006882	0.264206
-35.201815	-2.394197	2.731686	0.006876	0.264368
-34.689590	-2.459705	2.741683	0.006781	0.264519
-35.141138	-2.316670	2.751680	0.006865	0.264852
-34.559992	-2.384739	2.761677	0.006756	0.265058
-34.297753	-2.398752	2.771674	0.006708	0.265242
-34.064327	-2.392718	2.781670	0.006664	0.265507
-33.597962	-2.439308	2.791667	0.006577	0.265715
-34.012592	-2.327235	2.801664	0.006654	0.265915
-33.185242	-2.443448	2.811661	0.006500	0.266102
-33.395382	-2.349953	2.821658	0.006539	0.266402
-33.270989	-2.327229	2.831654	0.006516	0.266649
-32.991541	-2.337572	2.841651	0.006464	0.266868
-32.352165	-2.424968	2.851648	0.006345	0.267025
-31.776230	-2.473102	2.861645	0.006238	0.267332
-31.646124	-2.463633	2.871642	0.006214	0.267511
-31.976901	-2.363596	2.881638	0.006275	0.267727
-31.603691	-2.378576	2.891635	0.006206	0.268013
-31.778017	-2.298578	2.901632	0.006238	0.268274
-31.522126	-2.295498	2.911629	0.006191	0.268542
-31.422860	-2.271751	2.921626	0.006172	0.268767
-31.159844	-2.273504	2.931622	0.006123	0.269015
-30.802763	-2.289457	2.941619	0.006057	0.269279
-30.418622	-2.307677	2.951616	0.005985	0.269556
-30.163440	-2.308280	2.961613	0.005938	0.269802
-30.130735	-2.268319	2.971610	0.005931	0.270049
-29.856408	-2.273271	2.981606	0.005880	0.270290
-29.314998	-2.322224	2.991603	0.005780	0.270555
-29.531553	-2.234066	3.001600	0.005820	0.270816
-28.883387	-2.305147	3.011597	0.005699	0.271066
-28.875196	-2.263106	3.021594	0.005698	0.271298
-28.392710	-2.310066	3.031590	0.005608	0.271516
-28.744403	-2.190709	3.041587	0.005673	0.271811
-27.897111	-2.299117	3.051584	0.005516	0.272054
-27.467689	-2.326356	3.061581	0.005436	0.272325
-27.875077	-2.205674	3.071578	0.005511	0.272573
-26.959705	-2.329538	3.081574	0.005341	0.272799
-26.652767	-2.343556	3.091571	0.005284	0.273021
-26.829931	-2.254435	3.101568	0.005317	0.273322
-26.034874	-2.353551	3.111565	0.005169	0.273563
-26.354077	-2.251488	3.121562	0.005228	0.273796
-25.348661	-2.398851	3.131558	0.005041	0.273983
-25.434478	-2.328931	3.141555	0.005057	0.274270
-25.375615	-2.290282	3.151552	0.005046	0.274531
-25.215818	-2.272222	3.161549	0.005016	0.274779
-24.751548	-2.315843	3.171546	0.004930	0.274994
-24.202227	-2.375062	3.181542	0.004828	0.275208
-24.238703	-2.304616	3.191539	0.004834	0.275544
-23.813017	-2.351095	3.201536	0.004755	0.275706
-23.781630	-2.318640	3.211533	0.004749	0.275906
-23.555261	-2.316215	3.221530	0.004707	0.276135
-23.378649	-2.292691	3.231526	0.004674	0.276427
-23.169151	-2.279879	3.241523	0.004635	0.276693
-23.120669	-2.243249	3.251520	0.004626	0.276931
-22.745515	-2.266468	3.261517	0.004556	0.277166
-22.203016	-2.324989	3.271514	0.004455	0.277376
-22.160323	-2.271759	3.281510	0.004447	0.277694
-21.421052	-2.362210	3.291507	0.004310	0.277923
-21.016572	-2.398081	3.301504	0.004234	0.278119
-21.529193	-2.259410	3.311501	0.004330	0.278356
-21.555464	-2.196974	3.321498	0.004335	0.278655
-21.414999	-2.166100	3.331494	0.004308	0.278948
-21.059240	-2.178932	3.341491	0.004242	0.279217
-20.331469	-2.266362	3.351488	0.004107	0.279450
-20.363225	-2.216283	3.361485	0.004113	0.279680
-19.604203	-2.311664	3.371482	0.003971	0.279900
-19.651031	-2.242358	3.381478	0.003980	0.280214
-19.004735	-2.313305	3.391475	0.003860	0.280455
-18.811834	-2.311995	3.401472	0.003824	0.280643
-18.631468	-2.313543	3.411469	0.003790	0.280804
-18.224282	-2.330131	3.421466	0.003714	0.281100
-17.981091	-2.331870	3.431462	0.003669	0.281318
-18.228164	-2.242571	3.441459	0.003715	0.281547
-17.673271	-2.297205	3.451456	0.003612	0.281784
-17.394686	-2.298841	3.461453	0.003560	0.282036
-16.884195	-2.344499	3.471450	0.003465	0.282278
-16.639114	-2.352345	3.481446	0.003419	0.282466
-16.448859	-2.344383	3.491443	0.003384	0.282684
-16.052974	-2.352982	3.501440	0.003310	0.283009
-16.254562	-2.276541	3.511437	0.003348	0.283212
-16.082241	-2.265588	3.521434	0.003315	0.283428
-15.935990	-2.244708	3.531430	0.003288	0.283671
-15.451722	-2.279920	3.541427	0.003198	0.283940
-15.124168	-2.285567	3.551424	0.003137	0.284215
-14.866216	-2.290637	3.561421	0.003089	0.284428
-14.496248	-2.321866	3.571418	0.003020	0.284611
-14.395390	-2.286237	3.581414	0.003001	0.284885
-13.932680	-2.317676	3.591411	0.002915	0.285153
-13.769626	-2.305472	3.601408	0.002885	0.285365
-13.706865	-2.270511	3.611405	0.002873	0.285600
-13.357974	-2.294211	3.621402	0.002808	0.285802
-13.072074	-2.294734	3.631398	0.002755	0.286062
-13.132789	-2.239255	3.641395	0.002766	0.286287
-12.762581	-2.257408	3.651392	0.002697	0.286535
-12.228564	-2.310574	3.661389	0.002598	0.286757
-12.589853	-2.186759	3.671386	0.002665	0.287050
-12.102305	-2.227945	3.681382	0.002574	0.287290
-11.890503	-2.219551	3.691379	0.002535	0.287526
-11.634718	-2.219001	3.701376	0.002487	0.287762
-11.361648	-2.214350	3.711373	0.002436	0.288035
-10.865546	-2.251456	3.721370	0.002344	0.288302
-10.971043	-2.187179	3.731366	0.002364	0.288528
-10.622272	-2.203878	3.741363	0.002299	0.288763
-10.382727	-2.198891	3.751360	0.002254	0.289006
-10.121755	-2.187955	3.761357	0.002205	0.289298
-9.966679	-2.167592	3.771354	0.002177	0.289541
-10.145886	-2.081361	3.781350	0.002210	0.289809
-9.486109	-2.149671	3.791347	0.002087	0.290067
-8.885138	-2.216774	3.801344	0.001975	0.290277
-9.033405	-2.130535	3.811341	0.002003	0.290572
-8.644792	-2.154380	3.821338	0.001930	0.290805
-8.302456	-2.169411	3.831334	0.001867	0.291040
-8.329113	-2.118281	3.841331	0.001872	0.291270
-7.879337	-2.153590	3.851328	0.001788	0.291501
-6.953719	-2.268916	3.861325	0.001616	0.291763
-7.447685	-2.130450	3.871322	0.001707	0.292005
-6.472590	-2.263590	3.881318	0.001526	0.292223
-6.785651	-2.165271	3.891315	0.001584	0.292428
-6.601960	-2.144571	3.901312	0.001550	0.292696
-6.357414	-2.124048	3.911309	0.001504	0.293017
-6.093856	-2.127741	3.921306	0.001455	0.293235
-5.338323	-2.227057	3.931302	0.001315	0.293423
-5.313423	-2.190515	3.941299	0.001310	0.293625
-5.050719	-2.175051	3.951296	0.001261	0.293937
-5.326103	-2.074589	3.961293	0.001312	0.294185
-5.261199	-2.038971	3.971290	0.001300	0.294418
-4.211895	-2.186982	3.981286	0.001105	0.294628
-4.246044	-2.128489	3.991283	0.001111	0.294885
-3.918520	-2.126674	4.001280	0.001050	0.295185
-3.892061	-2.083182	4.011277	0.001045	0.295422
-3.568356	-2.101917	4.021274	0.000985	0.295618
-3.292001	-2.110278	4.031270	0.000934	0.295823
-4.276160	-1.868268	4.041267	0.001117	0.296132
-3.605188	-1.927393	4.051264	0.000992	0.296439
-3.750691	-1.839201	4.061261	0.001019	0.296740
-2.875811	-1.943524	4.071258	0.000856	0.297007
-3.442595	-1.781195	4.081254	0.000961	0.297296
-2.955268	-1.807828	4.091251	0.000871	0.297597
-3.535196	-1.632652	4.101248	0.000978	0.297936
-2.730815	-1.718223	4.111245	0.000829	0.298230
-2.354198	-1.727532	4.121242	0.000759	0.298517
-2.067372	-1.721155	4.131238	0.000705	0.298801
-2.204320	-1.629138	4.141235	0.000731	0.299125
-2.023506	-1.595858	4.151232	0.000697	0.299445
-2.253789	-1.486314	4.161229	0.000740	0.299772
-2.103010	-1.441017	4.171226	0.000712	0.300123
-2.275727	-1.330642	4.181222	0.000744	0.300504
-2.218165	-1.280230	4.191219	0.000733	0.300797
-2.047585	-1.227884	4.201216	0.000701	0.301197
-2.194122	-1.126370	4.211213	0.000728	0.301557
-2.187346	-1.047136	4.221210	0.000727	0.301943
-2.324082	-0.941736	4.231206	0.000752	0.302328
-1.134382	-1.071867	4.241203	0.000531	0.302740
-1.077466	-1.001456	4.251200	0.000520	0.303126
-1.284460	-0.884189	4.261197	0.000559	0.303506
-0.678033	-0.918628	4.271194	0.000446	0.303867
-1.162704	-0.736583	4.281190	0.000536	0.304314
-0.967278	-0.688538	4.291187	0.000500	0.304711
-0.554693	-0.676692	4.301184	0.000423	0.305123
-0.478636	-0.598266	4.311181	0.000409	0.305560
-0.630059	-0.485208	4.321178	0.000437	0.305965
-0.353990	-0.453123	4.331174	0.000385	0.306354
0.095739	-0.434429	4.341171	0.000302	0.306827
0.282475	-0.386164	4.351168	0.000267	0.307215
-0.286196	-0.185714	4.361165	0.000372	0.307672
-0.450382	-0.046205	4.371162	0.000403	0.308187
-0.158109	-0.005246	4.381158	0.000349	0.308629
0.000000	0.066436	4.391155	0.000319	0.309099

-0.078126	0.346459	4.396160	0.000333	0.310341
0.453874	0.807864	4.401165	0.000234	0.312932
1.378960	1.488675	4.406170	0.000061	0.316832
1.667191	2.578861	4.411174	0.000007	0.322007
1.776668	3.995637	4.416179	-0.000014	0.328399
3.068130	5.484941	4.421184	-0.000256	0.335907
4.182841	7.319866	4.426189	-0.000465	0.344570
4.954294	9.532866	4.431194	-0.000610	0.354312
7.296485	11.767404	4.436198	-0.001047	0.365009
9.992322	14.282196	4.441203	-0.001551	0.376724
11.780118	17.304050	4.446208	-0.001886	0.389360
13.134718	20.752682	4.451213	-0.002140	0.402849
15.815570	24.313304	4.456218	-0.002642	0.417123
24.469338	27.188025	4.461222	-0.004255	0.432245
26.266495	31.706542	4.466227	-0.004592	0.448155
28.019241	36.589243	4.471232	-0.004922	0.464628
34.039158	41.081324	4.476237	-0.006046	0.481677
40.220094	45.959328	4.481242	-0.007200	0.499340
45.055822	51.481779	4.486246	-0.008104	0.517519
47.367122	57.824589	4.491251	-0.008538	0.536062
50.862042	64.291416	4.496256	-0.009193	0.554862
57.862882	70.507145	4.501261	-0.010501	0.573998
62.112802	77.571484	4.506266	-0.011297	0.593373
64.976011	85.184676	4.511270	-0.011835	0.612840
69.487598	92.798737	4.516275	-0.012680	0.632382
74.315327	100.646028	4.521280	-0.013584	0.651975
82.616775	108.177820	4.526285	-0.015135	0.671649
88.430309	116.432714	4.531290	-0.016223	0.691339
90.953912	125.495048	4.536294	-0.016698	0.710926
96.718247	134.157442	4.541299	-0.017777	0.730336
100.732070	143.333997	4.546304	-0.018531	0.749628
104.910234	152.604292	4.551309	-0.019315	0.768664
109.292476	161.985428	4.556314	-0.020137	0.787505
113.974809	171.406893	4.561318	-0.021015	0.806069
122.552472	180.295418	4.566323	-0.022618	0.824484
127.481789	189.930564	4.571328	-0.023542	0.842664
133.264997	199.473220	4.576333	-0.024625	0.860554
143.696914	208.294254	4.581338	-0.026573	0.878233
148.689046	218.148688	4.586342	-0.027509	0.895678
152.474900	228.232094	4.591347	-0.028221	0.912814
156.506073	238.207794	4.596352	-0.028978	0.929530
161.959813	247.951707	4.601357	-0.030000	0.945974
167.613640	257.636878	4.606362	-0.031059	0.962096
172.026546	267.531078	4.611366	-0.031887	0.977938
179.552954	276.848404	4.616371	-0.033294	0.993474
201.479713	283.757823	4.621376	-0.037381	1.008904
215.348765	292.348981	4.626381	-0.039970	1.024482
254.679428	296.695440	4.631386	-0.047296	1.040052
283.683534	303.642776	4.636390	-0.052701	1.056470
284.739064	315.346510	4.641395	-0.052905	1.072514
285.645980	326.770537	4.646400	-0.053081	1.087919
287.027387	337.854395	4.651405	-0.053346	1.102770
287.985246	348.728437	4.656410	-0.053531	1.117060
289.291101	359.316873	4.661414	-0.053781	1.130882
290.801507	369.674743	4.666419	-0.054069	1.144291
292.071493	379.867749	4.671424	-0.054312	1.157287
292.624341	389.988711	4.676429	-0.054422	1.169900
293.742803	399.812637	4.681434	-0.054637	1.182134
297.712614	409.052439	4.686438	-0.055382	1.194124
300.281536	418.437877	4.691443	-0.055866	1.205882
302.257176	427.806653	4.696448	-0.056240	1.217386
303.242124	437.258442	4.701453	-0.056430	1.228682
304.379391	446.522666	4.706458	-0.056648	1.239687
305.144188	455.789042	4.711462	-0.056796	1.250525
307.028303	464.742909	4.716467	-0.057153	1.261129
310.230510	473.441836	4.721472	-0.057755	1.271607
312.148967	482.306905	4.726477	-0.058118	1.281941
313.622614	491.191147	4.731482	-0.058398	1.292130
315.077313	500.002459	4.736486	-0.058674	1.302154
316.389159	508.841648	4.741491	-0.058924	1.312105
317.270827	517.659011	4.746496	-0.059094	1.321879
318.506236	526.338377	4.751501	-0.059330	1.331496
319.927070	534.914970	4.756506	-0.059600	1.340966
321.711687	543.440988	4.761510	-0.059938	1.350380
323.496472	551.934268	4.766515	-0.060276	1.359694
324.970805	560.435407	4.771520	-0.060556	1.368897
326.047122	568.999523	4.776525	-0.060762	1.378035
327.360156	577.484556	4.781530	-0.061012	1.387071
328.490760	585.995090	4.786534	-0.061228	1.396043
330.154494	594.365118	4.791539	-0.061543	1.404904
331.612392	602.786376	4.796544	-0.061820	1.413726
333.201511	611.164499	4.801549	-0.062122	1.422471
334.069400	619.644787	4.806554	-0.062289	1.431145
335.608221	627.969577	4.811558	-0.062581	1.439722
336.747992	636.375979	4.816563	-0.062798	1.448263
337.904801	644.750080	4.821568	-0.063019	1.456724
338.860047	653.151921	4.826573	-0.063203	1.465131
340.001218	661.532658	4.831578	-0.063420	1.473499
341.481039	669.790582	4.836582	-0.063701	1.481754
343.336357	678.027333	4.841587	-0.064052	1.490001
345.094984	686.284240	4.846592	-0.064385	1.498206
346.062115	694.651425	4.851597	-0.064571	1.506348
346.790412	703.036141	4.856602	-0.064712	1.514425
347.538026	711.388620	4.861606	-0.064856	1.522432
348.057941	719.773708	4.866611	-0.064959	1.530392
348.423203	728.167236	4.871616	-0.065032	1.538295
349.197313	736.464564	4.876621	-0.065182	1.546130
350.175169	744.701632	4.881626	-0.065369	1.553901
351.340782	752.895560	4.886630	-0.065591	1.561620
352.136093	761.183385	4.891635	-0.065745	1.569332
352.961661	769.449601	4.896640	-0.065904	1.576991
353.719705	777.711216	4.901645	-0.066051	1.584599
354.406773	785.989069	4.906650	-0.066184	1.592174
355.539978	794.153420	4.911654	-0.066400	1.599676
356.193334	802.429881	4.916659	-0.066527	1.607173
356.679669	810.715687	4.921664	-0.066623	1.614620
357.138174	818.988866	4.926669	-0.066714	1.622017
357.434931	827.291538	4.931674	-0.066775	1.629384
358.146161	835.515304	4.936678	-0.066913	1.636707
358.419965	843.781489	4.941683	-0.066969	1.643973
358.978875	851.968493	4.946688	-0.067078	1.651177
359.616640	860.178457	4.951693	-0.067202	1.658380
360.033549	868.374628	4.956698	-0.067285	1.665510
360.810561	876.546466	4.961702	-0.067435	1.672638
361.877820	884.644541	4.966707	-0.067639	1.679712
362.597239	892.826475	4.971712	-0.067779	1.686780
363.259098	901.053948	4.976717	-0.067907	1.693849
363.648589	909.269259	4.981722	-0.067985	1.700841
365.044230	917.334110	4.986726	-0.068250	1.707812
365.507036	925.583344	4.991731	-0.068342	1.714786
366.009287	933.775570	4.996736	-0.068441	1.721689
366.709807	941.967791	5.001741	-0.068576	1.728590
367.211100	950.164170	5.006746	-0.068675	1.735440
368.067906	958.300153	5.011750	-0.068840	1.742260
368.902442	966.459089	5.016755	-0.069001	1.749069
369.660534	974.609910	5.021760	-0.069147	1.755835
370.761110	982.710079	5.026765	-0.069357	1.762577
371.131336	990.927908	5.031770	-0.069432	1.769296
371.877996	999.096457	5.036774	-0.069576	1.775997
372.838299	1007.213488	5.041779	-0.069760	1.782657
373.564900	1015.386903	5.046784	-0.069901	1.789309
374.181823	1023.600892	5.051789	-0.070021	1.795955
374.819857	1031.756507	5.056794	-0.070145	1.802532
375.536362	1039.917605	5.061798	-0.070284	1.809099
376.207737	1048.076129	5.066803	-0.070414	1.815634
376.567495	1056.268229	5.071808	-0.070486	1.822135
377.474223	1064.362948	5.076813	-0.070661	1.828602
377.686187	1072.572899	5.081818	-0.070705	1.835052
378.608793	1080.659284	5.086822	-0.070882	1.841468
378.689549	1088.908594	5.091827	-0.070903	1.847888
379.595419	1096.971394	5.096832	-0.071077	1.854240
380.194999	1105.117972	5.101837	-0.071194	1.860598
381.019020	1113.219805	5.106842	-0.071352	1.866926
381.882515	1121.323682	5.111846	-0.071519	1.873238
382.467441	1129.465300	5.116851	-0.071633	1.879525
383.088749	1137.594279	5.121856	-0.071754	1.885786
383.340014	1145.833191	5.126861	-0.071806	1.892067
383.850217	1153.954080	5.131866	-0.071906	1.898267
384.098980	1162.136743	5.136870	-0.071958	1.904464
384.807795	1170.234269	5.141875	-0.072095	1.910629
385.033251	1178.391965	5.146880	-0.072142	1.916764
385.571794	1186.522157	5.151885	-0.072248	1.922894
386.151965	1194.630274	5.156890	-0.072361	1.928993
386.482734	1202.796324	5.161894	-0.072428	1.935087
386.864500	1210.935711	5.166899	-0.072505	1.941148
387.782834	1218.963080	5.171904	-0.072681	1.947168
388.426497	1227.104838	5.176909	-0.072806	1.953222
388.322291	1235.294649	5.181914	-0.072792	1.959210
389.054901	1243.345248	5.186918	-0.072934	1.965170
389.374882	1251.502470	5.191923	-0.072999	1.971144
390.239388	1259.534399	5.196928	-0.073165	1.977068
390.826709	1267.673177	5.201933	-0.073279	1.983022
391.749072	1275.731939	5.206938	-0.073456	1.988936
392.333829	1283.847077	5.211942	-0.073571	1.994836
392.987251	1291.940145	5.216947	-0.073697	2.000711
393.801968	1299.997980	5.221952	-0.073854	2.006560
393.727422	1308.269153	5.226957	-0.073846	2.012450
394.090044	1316.391578	5.231962	-0.073919	2.018263
395.225878	1324.388516	5.236966	-0.074135	2.024051
396.257112	1332.449744	5.241971	-0.074333	2.029857
396.214179	1340.670998	5.246976	-0.074330	2.035647
396.700521	1348.767826	5.251981	-0.074426	2.041389
397.356070	1356.829289	5.256986	-0.074553	2.047106
397.824591	1364.950269	5.261990	-0.074646	2.052830
398.196915	1373.100355	5.266995	-0.074720	2.058548
398.210388	1381.261461	5.272000	-0.074728	2.064222
398.642373	1389.379293	5.277005	-0.074814	2.069892
398.517811	1397.546813	5.282010	-0.074796	2.075525
399.530353	1405.499278	5.287014	-0.074990	2.081109
399.964824	1413.618199	5.292019	-0.075076	2.086734
400.152991	1421.763094	5.297024	-0.075116	2.092337
400.845143	1429.838672	5.302029	-0.075251	2.097928
401.831126	1437.834566	5.307034	-0.075439	2.103478
402.510246	1445.943273	5.312038	-0.075571	2.109060
402.523708	1454.182356	5.317043	-0.075579	2.114650
402.935042	1462.227262	5.322048	-0.075661	2.120133
404.401384	1470.144726	5.327053	-0.075939	2.125619
404.951319	1478.261191	5.332058	-0.076047	2.131135
405.668695	1486.330546	5.337062	-0.076186	2.136621
405.612118	1494.565163	5.342067	-0.076180	2.142129
406.170221	1502.615911	5.347072	-0.076290	2.147559
406.633837	1510.738565	5.352077	-0.076381	2.153014
406.986696	1518.821126	5.357082	-0.076452	2.158418
407.647121	1526.859499	5.362086	-0.076580	2.163808
407.988039	1535.000219	5.367091	-0.076649	2.169223
407.901050	1543.173741	5.372096	-0.076638	2.174605
408.319671	1551.255083	5.377101	-0.076721	2.179960
408.898237	1559.275294	5.382106	-0.076834	2.185277
408.944266	1567.446250	5.387110	-0.076848	2.190630
409.516211	1575.479622	5.392115	-0.076960	2.195929
409.907125	1583.527760	5.397120	-0.077038	2.201208
410.469297	1591.591265	5.402125	-0.077148	2.206500
410.795420	1599.692459	5.407130	-0.077214	2.211782
411.141283	1607.790433	5.412134	-0.077284	2.217051
411.095412	1615.952683	5.417139	-0.077280	2.222314
411.043216	1624.095818	5.422144	-0.077276	2.227551
411.498531	1632.134997	5.427149	-0.077366	2.232754
411.690218	1640.225116	5.432154	-0.077407	2.237955
412.010689	1648.257005	5.437158	-0.077472	2.243117
412.451378	1656.335923	5.442163	-0.077559	2.248309
412.471930	1664.442891	5.447168	-0.077568	2.253469
413.143891	1672.456224	5.452173	-0.077699	2.258615
413.571173	1680.518198	5.457178	-0.077784	2.263759
414.487244	1688.540761	5.462182	-0.077959	2.268909
414.957682	1696.683005	5.467187	-0.078052	2.274083
415.471608	1704.705692	5.472192	-0.078153	2.279174
416.164902	1712.731820	5.477197	-0.078288	2.284272
416.746303	1720.795341	5.482202	-0.078401	2.289371
416.752242	1728.953203	5.487206	-0.078407	2.294469
417.681469	1736.959585	5.492211	-0.078586	2.299540
418.183214	1744.996920	5.497216	-0.078684	2.304582
418.533021	1753.120441	5.502221	-0.078755	2.309654
418.519300	1761.281438	5.507226	-0.078758	2.314707
419.367443	1769.265518	5.512230	-0.078921	2.319712
419.502713	1777.396180	5.517235	-0.078951	2.324737
419.969624	1785.430893	5.522240	-0.079043	2.329720
420.621872	1793.507483	5.527245	-0.079170	2.334733
421.066790	1801.575558	5.532250	-0.079258	2.339713
421.397981	1809.651051	5.537254	-0.079325	2.344677
421.724536	1817.778855	5.542259	-0.079391	2.349662
422.455853	1825.765012	5.547264	-0.079533	2.354583
422.820239	1833.869806	5.552269	-0.079606	2.359537
423.333708	1841.903406	5.557274	-0.079707	2.364448
423.743496	1850.000883	5.562278	-0.079788	2.369380
424.365033	1858.049421	5.567283	-0.079909	2.374289
424.872573	1866.085264	5.572288	-0.080009	2.379170
425.440682	1874.151653	5.577293	-0.080120	2.384065
425.777998	1882.243605	5.582298	-0.080188	2.388947
425.798136	1890.394357	5.587302	-0.080197	2.393828
426.582065	1898.393588	5.592307	-0.080348	2.398669
427.403407	1906.362579	5.597312	-0.080506	2.403486
427.730966	1914.495443	5.602317	-0.080573	2.408351
428.036012	1922.600618	5.607322	-0.080635	2.413188
428.600227	1930.634245	5.612326	-0.080745	2.417994
428.758560	1938.770152	5.617331	-0.080780	2.422818
429.102455	1946.823905	5.622336	-0.080849	2.427599
429.881536	1954.891008	5.627341	-0.080999	2.432412
430.754480	1962.884852	5.632346	-0.081167	2.437179
431.133638	1970.931143	5.637350	-0.081243	2.441930
431.424949	1979.053512	5.642355	-0.081303	2.446709
431.830993	1987.120440	5.647360	-0.081383	2.451455
432.401398	1995.166924	5.652365	-0.081495	2.456193
432.777441	2003.219961	5.657370	-0.081570	2.460910
432.767344	2011.371070	5.662374	-0.081574	2.465645
433.506181	2019.364353	5.667379	-0.081716	2.470337
434.176321	2027.366373	5.672384	-0.081846	2.475020
434.158291	2035.530890	5.677389	-0.081848	2.479736
434.666930	2043.507359	5.682394	-0.081948	2.484374
434.985879	2051.592708	5.687398	-0.082013	2.489051
434.891809	2059.760753	5.692403	-0.082001	2.493736
434.864176	2067.862190	5.697408	-0.082001	2.498380
435.054825	2075.919289	5.702413	-0.082042	2.503005
435.557595	2083.918226	5.707418	-0.082140	2.507612
435.814746	2091.987489	5.712422	-0.082194	2.512232
436.053742	2100.048867	5.717427	-0.082243	2.516838
436.494992	2108.042198	5.722432	-0.082331	2.521412
436.993145	2116.087921	5.727437	-0.082429	2.526011
437.286061	2124.170839	5.732442	-0.082489	2.530608
437.337792	2132.276889	5.737446	-0.082503	2.535191
437.724958	2140.325633	5.742451	-0.082581	2.539759
438.394778	2148.269738	5.747456	-0.082711	2.544280
439.145116	2156.315152	5.752461	-0.082856	2.548855
438.816281	2164.484020	5.757466	-0.082800	2.553414
439.418279	2172.486108	5.762470	-0.082917	2.557937
440.123527	2180.510314	5.767475	-0.083054	2.562473
440.639893	2188.486891	5.772480	-0.083155	2.566960
441.103093	2196.601174	5.777485	-0.083246	2.571512
441.184488	2204.720230	5.782490	-0.083267	2.576032
441.742301	2212.734077	5.787494	-0.083376	2.580519
441.765825	2220.852960	5.792499	-0.083386	2.585019
442.322031	2228.884244	5.797504	-0.083494	2.589500
442.400325	2237.110942	5.802509	-0.083514	2.594047
442.710037	2245.103134	5.807514	-0.083577	2.598474
442.953117	2253.135383	5.812518	-0.083628	2.602910
443.647210	2261.105471	5.817523	-0.083762	2.607335
444.108447	2269.114325	5.822528	-0.083853	2.611758
444.565208	2277.167284	5.827533	-0.083944	2.616198
445.601567	2285.104039	5.832538	-0.084142	2.620605
445.624979	2293.232487	5.837542	-0.084151	2.625041
445.738608	2301.363515	5.842547	-0.084178	2.629477
446.165701	2309.397114	5.847552	-0.084263	2.633874
446.454078	2317.467023	5.852557	-0.084322	2.638273
446.989540	2325.452036	5.857562	-0.084427	2.642636
447.797619	2333.422743	5.862566	-0.084582	2.647002
448.043200	2341.563979	5.867571	-0.084633	2.651415
448.318204	2349.622307	5.872576	-0.084690	2.655778
448.323584	2357.752677	5.877581	-0.084696	2.660154
449.237064	2365.684636	5.882586	-0.084871	2.664477
449.787206	2373.742013	5.887590	-0.084979	2.668836
449.877880	2381.859659	5.892595	-0.085001	2.673190
449.956695	2389.922518	5.897600	-0.085021	2.677507
450.737143	2397.898428	5.902605	-0.085172	2.681816
451.151503	2405.932112	5.907610	-0.085254	2.686125
451.364515	2414.022160	5.912614	-0.085299	2.690444
451.844795	2422.099445	5.917619	-0.085394	2.694766
452.179625	2430.100962	5.922624	-0.085461	2.699032
451.966643	2438.253443	5.927629	-0.085427	2.703336
452.489606	2446.246792	5.932634	-0.085529	2.707596
452.886017	2454.288983	5.937638	-0.085608	2.711867
453.204264	2462.357630	5.942643	-0.085673	2.716140
453.666017	2470.338849	5.947648	-0.085764	2.720369
454.375849	2478.340523	5.952653	-0.085902	2.724619
454.559838	2486.429279	5.957658	-0.085941	2.728874
454.821802	2494.515505	5.962662	-0.085995	2.733125
455.102961	2502.611599	5.967667	-0.086053	2.737377
455.494097	2510.603853	5.972672	-0.086131	2.741574
455.775839	2518.683305	5.977677	-0.086189	2.745804
456.117219	2526.759312	5.982682	-0.086257	2.750029
456.809874	2534.788337	5.987686	-0.086392	2.754245
457.467651	2542.767361	5.992691	-0.086519	2.758426
457.378571	2550.834912	5.997696	-0.086508	2.762600
457.529320	2558.929259	6.002701	-0.086541	2.766797
458.025583	2566.931258	6.007706	-0.086639	2.770961
458.368411	2574.982977	6.012710	-0.086708	2.775135
458.581578	2583.058573	6.017715	-0.086753	2.779307
459.032570	2591.030517	6.022720	-0.086842	2.783434
459.258439	2599.115077	6.027725	-0.086889	2.787598
459.608018	2607.154175	6.032730	-0.086960	2.791741
460.053943	2615.181390	6.037734	-0.087048	2.795877
460.369713	2623.224262	6.042739	-0.087112	2.800007
460.558067	2631.218686	6.047744	-0.087152	2.804099
461.183144	2639.273634	6.052749	-0.087274	2.808241
461.593485	2647.333123	6.057754	-0.087356	2.812367
461.583793	2655.458079	6.062758	-0.087359	2.816495
462.480849	2663.427074	6.067763	-0.087531	2.820591
462.749232	2671.475535	6.072768	-0.087587	2.824685
463.329581	2679.525331	6.077773	-0.087700	2.828791
463.654144	2687.555868	6.082778	-0.087766	2.832867
463.791108	2695.636965	6.087782	-0.087796	2.836951
464.880629	2703.602382	6.092787	-0.088004	2.841026
464.987550	2711.644067	6.097792	-0.088030	2.845078
465.283267	2719.727417	6.102797	-0.088090	2.849155
465.442079	2727.823748	6.107802	-0.088125	2.853224
465.344074	2735.910965	6.112806	-0.088112	2.857269
466.456829	2743.825011	6.117811	-0.088324	2.861290
466.904408	2751.814121	6.122816	-0.088413	2.865306
467.346286	2759.904918	6.127821	-0.088500	2.869366
466.989887	2768.044655	6.132826	-0.088439	2.873399
466.813747	2776.135165	6.137830	-0.088412	2.877413
467.331386	2784.137610	6.142835	-0.088513	2.881416
467.792927	2792.089723	6.147840	-0.088604	2.885385
468.251412	2800.151170	6.152845	-0.088695	2.889403
468.595834	2808.226726	6.157850	-0.088764	2.893416
468.941241	2816.274991	6.162854	-0.088834	2.897409
469.492896	2824.274229	6.167859	-0.088942	2.901384
469.477093	2832.349050	6.172864	-0.088944	2.905360
470.155402	2840.345259	6.177869	-0.089076	2.909330
470.572964	2848.452236	6.182874	-0.089159	2.913334
470.535566	2856.529146	6.187878	-0.089157	2.917294
471.310294	2864.507669	6.192883	-0.089307	2.921243
471.702113	2872.499334	6.197888	-0.089385	2.925173
472.624597	2880.448762	6.202893	-0.089562	2.929106
472.785506	2888.544804	6.207898	-0.089597	2.933063
473.174706	2896.596093	6.212902	-0.089675	2.937006
473.701664	2904.630517	6.217907	-0.089778	2.940943
473.862339	2912.703747	6.222912	-0.089813	2.944873
474.123950	2920.771067	6.227917	-0.089867	2.948801
474.366417	2928.828806	6.232922	-0.089917	2.952718
474.691841	2936.838019	6.237926	-0.089983	2.956610
475.360007	2944.842820	6.242931	-0.090113	2.960514
475.363747	2952.872782	6.247936	-0.090119	2.964389
475.397361	2960.975505	6.252941	-0.090130	2.968296
476.052567	2968.970682	6.257946	-0.090258	2.972178
476.044320	2977.072067	6.262950	-0.090261	2.976072
476.163438	2985.117030	6.267955	-0.090289	2.979940
476.550180	2993.077375	6.272960	-0.090366	2.983776
477.003389	3001.119363	6.277965	-0.090456	2.987650
477.148376	3009.228462	6.282970	-0.090488	2.991535
477.553043	3017.232203	6.287974	-0.090568	2.995378
478.297171	3025.195925	6.292979	-0.090712	2.999214
478.417473	3033.231885	6.297984	-0.090740	3.003048
478.474662	3041.350543	6.302989	-0.090756	3.006913
478.899114	3049.390205	6.307994	-0.090840	3.010754
479.032314	3057.423712	6.312998	-0.090870	3.014572
479.840828	3065.375219	6.318003	-0.091026	3.018381
480.164530	3073.397438	6.323008	-0.091091	3.022194
480.668058	3081.479160	6.328013	-0.091190	3.026039
480.794293	3089.556708	6.333018	-0.091219	3.029858
481.208207	3097.568050	6.338022	-0.091301	3.033656
481.694021	3105.606032	6.343027	-0.091397	3.037465
481.304169	3113.737643	6.348032	-0.091330	3.041270
481.367793	3121.754261	6.353037	-0.091347	3.045038
482.255746	3129.659311	6.358042	-0.091517	3.048790
482.136706	3137.798259	6.363046	-0.091501	3.052598
482.262423	3145.903976	6.368051	-0.091529	3.056397
482.635860	3153.863272	6.373056	-0.091604	3.060135
483.299459	3161.825357	6.378061	-0.091733	3.063883
483.314754	3169.922508	6.383066	-0.091741	3.067659
484.238795	3177.875997	6.388070	-0.091918	3.071407
484.623174	3186.002447	6.393075	-0.091995	3.075204
484.976321	3193.965462	6.398080	-0.092066	3.078920
485.369316	3202.010307	6.403085	-0.092144	3.082671
486.079943	3209.979549	6.408090	-0.092282	3.086397
486.148495	3218.085491	6.413094	-0.092300	3.090151
486.311815	3226.166038	6.418099	-0.092336	3.093894
486.352261	3234.233040	6.423104	-0.092348	3.097620
486.662826	3242.281128	6.428109	-0.092411	3.101346
487.095637	3250.252796	6.433114	-0.092497	3.105037
487.447717	3258.266074	6.438118	-0.092568	3.108739
488.194048	3266.273957	6.443123	-0.092712	3.112453
488.788411	3274.271634	6.448128	-0.092828	3.116150
488.622671	3282.385184	6.453133	-0.092803	3.119862
489.076016	3290.373465	6.458138	-0.092892	3.123539
489.348173	3298.406540	6.463142	-0.092948	3.127225
489.808390	3306.482511	6.468147	-0.093039	3.130934
490.112214	3314.480425	6.473152	-0.093101	3.134596
490.896342	3322.482762	6.478157	-0.093252	3.138278
490.804791	3330.612401	6.483162	-0.093240	3.141973
491.198132	3338.618491	6.488166	-0.093319	3.145630
491.922665	3346.596661	6.493171	-0.093459	3.149285
491.647419	3354.724099	6.498176	-0.093413	3.152958
492.047887	3362.744925	6.503181	-0.093493	3.156609
492.321987	3370.746885	6.508186	-0.093549	3.160241
492.511241	3378.768562	6.513190	-0.093589	3.163875
492.734330	3386.823945	6.518195	-0.093636	3.167521
493.121413	3394.821494	6.523200	-0.093713	3.171143
493.589042	3402.875365	6.528205	-0.093806	3.174791
493.864288	3410.879613	6.533210	-0.093862	3.178403
493.853643	3418.932591	6.538214	-0.093866	3.182021
494.669755	3426.928831	6.543219	-0.094023	3.185645
494.734515	3434.995144	6.548224	-0.094040	3.189264
494.700407	3443.105281	6.553229	-0.094039	3.192894
495.154873	3451.087654	6.558234	-0.094129	3.196483
495.700149	3459.083123	6.563238	-0.094236	3.200079
495.898984	3467.106974	6.568243	-0.094278	3.203668
496.101953	3475.161959	6.573248	-0.094321	3.207267
496.747588	3483.181864	6.578253	-0.094446	3.210865
496.606929	3491.270326	6.583258	-0.094425	3.214456
496.461456	3499.326740	6.588262	-0.094404	3.218029
496.786885	3507.379177	6.593267	-0.094469	3.221616
497.027469	3515.361378	6.598272	-0.094519	3.225164
497.344021	3523.390492	6.603277	-0.094584	3.228732
497.477396	3531.448696	6.608282	-0.094614	3.232301
497.885256	3539.438515	6.613286	-0.094695	3.235848
498.443139	3547.394948	6.618291	-0.094804	3.239382
498.661842	3555.431014	6.623296	-0.094850	3.242933
499.110465	3563.451023	6.628301	-0.094939	3.246483
499.153636	3571.547585	6.633306	-0.094952	3.250046
499.543865	3579.544766	6.638310	-0.095030	3.253575
499.731658	3587.624389	6.643315	-0.095070	3.257129
499.844426	3595.657166	6.648320	-0.095096	3.260655
500.594842	3603.605642	6.653325	-0.095241	3.264166
501.192125	3611.607854	6.658330	-0.095358	3.267690
501.826375	3619.632054	6.663334	-0.095481	3.271222
502.050307	3627.730762	6.668339	-0.095528	3.274766
501.966269	3635.794879	6.673344	-0.095518	3.278278
502.772223	3643.744077	6.678349	-0.095673	3.281772
502.579762	3651.856966	6.683354	-0.095642	3.285294
502.518733	3659.888905	6.688358	-0.095636	3.288783
502.721309	3667.981717	6.693363	-0.095679	3.292304
502.990912	3676.026094	6.698368	-0.095735	3.295803
503.585269	3683.935913	6.703373	-0.095850	3.299253
503.755661	3691.957462	6.708378	-0.095887	3.302731
504.408603	3699.940567	6.713382	-0.096014	3.306207
504.639631	3708.062832	6.718387	-0.096062	3.309723
504.901544	3716.073781	6.723392	-0.096116	3.313189
504.747117	3724.188422	6.728397	-0.096093	3.316680
505.475693	3732.104425	6.733402	-0.096234	3.320115
506.027945	3740.067907	6.738406	-0.096342	3.323561
505.358859	3748.322795	6.743411	-0.096223	3.327081
506.038103	3756.246194	6.748416	-0.096354	3.330507
506.708246	3764.210223	6.753421	-0.096484	3.333946
507.207449	3772.240178	6.758426	-0.096582	3.337403
507.008620	3780.361259	6.763430	-0.096551	3.340870
507.581156	3788.322870	6.768435	-0.096662	3.344293
507.472697	3796.403021	6.773440	-0.096648	3.347738
507.834763	3804.437171	6.778445	-0.096720	3.351178
508.267524	3812.438401	6.783450	-0.096806	3.354602
508.680071	3820.421151	6.788454	-0.096888	3.358015
509.240121	3828.447192	6.793459	-0.096998	3.361447
509.895897	3836.368982	6.798464	-0.097125	3.364836
510.397796	3844.452260	6.803469	-0.097224	3.368283
509.996566	3852.615982	6.808474	-0.097154	3.371729
510.523004	3860.589342	6.813478	-0.097257	3.375123
510.737942	3868.653093	6.818483	-0.097303	3.378542
510.877232	3876.698327	6.823488	-0.097334	3.381946
511.470953	3884.655221	6.828493	-0.097450	3.385326
511.837207	3892.720478	6.833498	-0.097523	3.388740
511.946603	3900.788441	6.838502	-0.097549	3.392142
512.316373	3908.837293	6.843507	-0.097623	3.395542
512.653267	3916.787950	6.848512	-0.097691	3.398897
512.873295	3924.804836	6.853517	-0.097737	3.402271
513.097249	3932.852541	6.858522	-0.097784	3.405655
513.034323	3940.902653	6.863526	-0.097777	3.409027
513.380964	3948.942801	6.868531	-0.097847	3.412406
513.648505	3956.962605	6.873536	-0.097902	3.415770
513.845961	3964.976112	6.878541	-0.097944	3.419125
514.521446	3972.925638	6.883546	-0.098075	3.422467
515.169122	3980.916277	6.888550	-0.098201	3.425822
515.656754	3988.974051	6.893555	-0.098297	3.429196
515.726267	3997.059538	6.898560	-0.098315	3.432564
516.066572	4005.128431	6.903565	-0.098384	3.435931
516.607733	4013.057300	6.908570	-0.098490	3.439243
516.956896	4021.065522	6.913574	-0.098560	3.442578
517.496750	4029.127855	6.918579	-0.098666	3.445939
517.681644	4037.152640	6.923584	-0.098705	3.449269
518.019694	4045.192428	6.928589	-0.098774	3.452607
518.048139	4053.319722	6.933594	-0.098784	3.455967
518.269341	4061.270657	6.938598	-0.098831	3.459258
518.274414	4069.383781	6.943603	-0.098837	3.462606
518.160928	4077.418086	6.948608	-0.098821	3.465913
518.601182	4085.419255	6.953613	-0.098908	3.469223
519.497703	4093.346094	6.958618	-0.099080	3.472513
519.433924	4101.445176	6.963622	-0.099074	3.475840
520.205262	4109.389432	6.968627	-0.099222	3.479127
520.288328	4117.435247	6.973632	-0.099243	3.482430
520.407468	4125.518654	6.978637	-0.099271	3.485747
520.651692	4133.523612	6.983642	-0.099321	3.489032
521.262851	4141.513322	6.988646	-0.099440	3.492320
521.741512	4149.574050	6.993651	-0.099535	3.495629
522.587881	4157.458392	6.998656	-0.099697	3.498875
523.284315	4165.560577	7.003661	-0.099832	3.502202
523.315665	4173.651587	7.008666	-0.099843	3.505500
523.669456	4181.669809	7.013670	-0.099915	3.508775
523.891607	4189.753567	7.018675	-0.099961	3.512069
524.126611	4197.757929	7.023680	-0.100010	3.515329
524.244870	4205.748878	7.028685	-0.100037	3.518577
524.649701	4213.780564	7.033690	-0.100118	3.521847
525.285849	4221.756585	7.038694	-0.100242	3.525098
525.611769	4229.788831	7.043699	-0.100308	3.528360
525.866877	4237.872717	7.048704	-0.100360	3.531637
526.331063	4245.862427	7.053709	-0.100452	3.534879
526.399724	4253.937088	7.058714	-0.100470	3.538141
526.693596	4261.933936	7.063718	-0.100530	3.541375
527.224494	4269.905505	7.068723	-0.100634	3.544603
527.957717	4277.915821	7.073728	-0.100776	3.547850
527.790718	4286.089599	7.078733	-0.100750	3.551132
528.335120	4294.095213	7.083738	-0.100857	3.554365
528.338761	4302.108559	7.088742	-0.100862	3.557582
528.729311	4310.118852	7.093747	-0.100940	3.560807
528.548218	4318.097488	7.098752	-0.100912	3.563998
529.492276	4326.065606	7.103757	-0.101093	3.567217
529.678953	4334.150015	7.108762	-0.101133	3.570456
529.770487	4342.171537	7.113766	-0.101155	3.573664
530.072527	4350.259844	7.118771	-0.101217	3.576902
530.423108	4358.207182	7.123776	-0.101287	3.580082
530.655966	4366.240954	7.128781	-0.101336	3.583291
531.186634	4374.233510	7.133786	-0.101440	3.586489
531.620872	4382.291544	7.138790	-0.101526	3.589707
531.920302	4390.347211	7.143795	-0.101587	3.592917
532.183584	4398.371169	7.148800	-0.101641	3.596111
532.487663	4406.356125	7.153805	-0.101703	3.599288
532.575111	4414.437251	7.158810	-0.101725	3.602493
532.560846	4422.447002	7.163814	-0.101727	3.605665
532.777672	4430.495312	7.168819	-0.101773	3.608856
533.041073	4438.515113	7.173824	-0.101827	3.612033
533.222707	4446.543215	7.178829	-0.101866	3.615209
533.661604	4454.512599	7.183834	-0.101953	3.618367
534.145862	4462.531072	7.188838	-0.102048	3.621542
534.380752	4470.583249	7.193843	-0.102097	3.624720
534.365534	4478.625409	7.198848	-0.102100	3.627885
534.940722	4486.652734	7.203853	-0.102212	3.631058
535.333664	4494.638180	7.208858	-0.102290	3.634206
535.668601	4502.653906	7.213862	-0.102358	3.637362
536.053494	4510.708294	7.218867	-0.102435	3.640531
536.041450	4518.697183	7.223872	-0.102438	3.643661
536.604430	4526.694363	7.228877	-0.102548	3.646808
537.102506	4534.747138	7.233882	-0.102646	3.649971
537.294078	4542.765231	7.238886	-0.102687	3.653110
537.714126	4550.835320	7.243891	-0.102770	3.656273
537.918553	4558.803359	7.248896	-0.102814	3.659387
537.975286	4566.887785	7.253901	-0.102829	3.662540
538.345735	4574.907200	7.258906	-0.102904	3.665673
538.194777	4582.958828	7.263910	-0.102881	3.668802
538.746843	4591.005540	7.268915	-0.102989	3.671945
539.099733	4598.966798	7.273920	-0.103060	3.675047
539.092005	4607.010062	7.278925	-0.103064	3.678169
538.824558	4615.109913	7.283930	-0.103019	3.681303
539.304013	4623.003447	7.288934	-0.103113	3.684374
540.095463	4631.024831	7.293939	-0.103266	3.687500
540.386325	4639.043287	7.298944	-0.103325	3.690610
540.760564	4647.072776	7.303949	-0.103400	3.693723
540.716107	4655.190454	7.308954	-0.103397	3.696856
540.924101	4663.187358	7.313958	-0.103441	3.699947
541.201902	4671.209925	7.318963	-0.103498	3.703047
541.714686	4679.192226	7.323968	-0.103599	3.706134
541.716390	4687.279949	7.328973	-0.103605	3.709247
542.053526	4695.341112	7.333978	-0.103673	3.712355
541.987187	4703.393288	7.338982	-0.103665	3.715447
542.254162	4711.335238	7.343987	-0.103720	3.718503
542.454058	4719.340317	7.348992	-0.103763	3.721578
542.803040	4727.280520	7.353997	-0.103833	3.724630
543.272489	4735.353380	7.359002	-0.103926	3.727733
542.977843	4743.454623	7.364006	-0.103876	3.730825
542.893367	4751.508941	7.369011	-0.103866	3.733902
542.755783	4759.542200	7.374016	-0.103845	3.736968
543.610620	4767.462223	7.379021	-0.104010	3.740011
544.202787	4775.413978	7.384026	-0.104125	3.743058
544.179597	4783.488548	7.389030	-0.104126	3.746134
544.679852	4791.487444	7.394035	-0.104224	3.749191
544.341263	4799.598503	7.399040	-0.104167	3.752269
544.834421	4807.559472	7.404045	-0.104264	3.755307
545.265362	4815.571305	7.409050	-0.104349	3.758360
545.179572	4823.641860	7.414054	-0.104338	3.761420
545.067836	4831.685153	7.419059	-0.104323	3.764467
545.399885	4839.672765	7.424064	-0.104390	3.767501
545.750109	4847.692247	7.429069	-0.104460	3.770545
545.969923	4855.665306	7.434074	-0.104506	3.773566
546.372969	4863.698058	7.439078	-0.104587	3.776611
546.459510	4871.799046	7.444083	-0.104608	3.779672
546.793195	4879.738423	7.449088	-0.104675	3.782676
546.743741	4887.861667	7.454093	-0.104671	3.785737
547.280062	4895.855617	7.459098	-0.104776	3.788761
547.604150	4903.857412	7.464102	-0.104842	3.791780
548.065229	4911.866613	7.469107	-0.104933	3.794803
547.741372	4919.930395	7.474112	-0.104878	3.797826
548.839222	4927.821347	7.479117	-0.105088	3.800814
548.879457	4935.858701	7.484122	-0.105100	3.803830
549.653647	4943.856300	7.489126	-0.105250	3.806846
550.005629	4951.912302	7.494131	-0.105321	3.809871
550.089533	4959.973187	7.499136	-0.105341	3.812890
549.581410	4968.153039	7.504141	-0.105252	3.815938
549.974802	4976.054788	7.509146	-0.105331	3.818900
550.519074	4984.037662	7.514150	-0.105437	3.821892
551.328295	4992.011591	7.519155	-0.105593	3.824885
551.483795	5000.066138	7.524160	-0.105627	3.827891
551.527158	5008.183054	7.529165	-0.105641	3.830916
551.565805	5016.195085	7.534170	-0.105653	3.833899
551.635745	5024.248529	7.539174	-0.105671	3.836896
552.222255	5032.199695	7.544179	-0.105786	3.839863
552.362774	5040.207987	7.549184	-0.105817	3.842840
552.277396	5048.265720	7.554189	-0.105806	3.845828
552.421275	5056.347006	7.559194	-0.105838	3.848827
553.050745	5064.269795	7.564198	-0.105961	3.851776
553.245370	5072.313712	7.569203	-0.106002	3.854758
553.590031	5080.305707	7.574208	-0.106072	3.857721
554.457912	5088.286558	7.579213	-0.106238	3.860689
554.115740	5096.373542	7.584218	-0.106180	3.863668
555.001743	5104.326448	7.589222	-0.106350	3.866622
554.993843	5112.448813	7.594227	-0.106354	3.869617
555.078677	5120.573207	7.599232	-0.106375	3.872612
554.933570	5128.675009	7.604237	-0.106353	3.875592
555.167777	5136.562714	7.609242	-0.106402	3.878498
555.875689	5144.484107	7.614246	-0.106539	3.881425
556.621668	5152.413121	7.619251	-0.106683	3.884352
556.477557	5160.499640	7.624256	-0.106662	3.887317
556.704210	5168.524572	7.629261	-0.106709	3.890265
556.817471	5176.611224	7.634266	-0.106735	3.893231
556.712622	5184.662914	7.639270	-0.106721	3.896178
557.438744	5192.576421	7.644275	-0.106861	3.899088
557.637785	5200.630974	7.649280	-0.106904	3.902037
557.431960	5208.684972	7.654285	-0.106871	3.904975
558.088953	5216.693391	7.659290	-0.106998	3.907912
558.474658	5224.680453	7.664294	-0.107075	3.910833
558.625015	5232.737403	7.669299	-0.107109	3.913773
558.587201	5240.768301	7.674304	-0.107107	3.916698
559.377984	5248.665976	7.679309	-0.107259	3.919588
559.896379	5256.706735	7.684314	-0.107361	3.922522
559.961467	5264.739347	7.689318	-0.107378	3.925443
560.450584	5272.776801	7.694323	-0.107475	3.928371
560.571219	5280.852264	7.699328	-0.107502	3.931304
561.031334	5288.822607	7.704333	-0.107593	3.934202
561.298773	5296.886403	7.709338	-0.107648	3.937129
562.034674	5304.865311	7.714342	-0.107790	3.940032
562.418528	5312.887182	7.719347	-0.107867	3.942941
562.422028	5320.955865	7.724352	-0.107873	3.945858
562.968143	5328.966186	7.729357	-0.107980	3.948762
562.998559	5337.084497	7.734362	-0.107991	3.951693
563.158524	5345.030995	7.739366	-0.108026	3.954563
563.540535	5353.055529	7.744371	-0.108102	3.957462
564.016787	5361.011242	7.749376	-0.108196	3.960336
564.397053	5369.025379	7.754381	-0.108272	3.963228
564.329036	5377.137793	7.759386	-0.108265	3.966144
564.803557	5385.063761	7.764390	-0.108358	3.969001
564.988109	5393.186244	7.769395	-0.108398	3.971921
564.651632	5401.218124	7.774400	-0.108341	3.974798
565.267907	5409.153242	7.779405	-0.108460	3.977654
565.678719	5417.182613	7.784410	-0.108542	3.980539
565.811665	5425.184154	7.789414	-0.108572	3.983406
566.139715	5433.251204	7.794419	-0.108638	3.986299
566.530441	5441.211241	7.799424	-0.108716	3.989151
566.931475	5449.279804	7.804429	-0.108796	3.992041
566.975881	5457.337890	7.809434	-0.108810	3.994919
567.142919	5465.329555	7.814438	-0.108846	3.997773
567.235775	5473.392656	7.819443	-0.108869	4.000649
567.766805	5481.311562	7.824448	-0.108973	4.003480
568.449794	5489.288064	7.829453	-0.109105	4.006331
569.119010	5497.307172	7.834458	-0.109235	4.009194
569.177252	5505.394523	7.839462	-0.109251	4.012070
569.723203	5513.406587	7.844467	-0.109358	4.014925
570.007756	5521.401259	7.849472	-0.109416	4.017768
570.077401	5529.509153	7.854477	-0.109434	4.020645
570.249206	5537.531075	7.859482	-0.109472	4.023492
570.163085	5545.561487	7.864486	-0.109461	4.026335
571.098912	5553.500819	7.869491	-0.109640	4.029160
570.873628	5561.635393	7.874496	-0.109604	4.032034
570.978132	5569.678940	7.879501	-0.109628	4.034878
571.596369	5577.622504	7.884506	-0.109749	4.037694
572.315276	5585.546235	7.889510	-0.109888	4.040502
572.517085	5593.603699	7.894515	-0.109931	4.043347
572.681611	5601.654371	7.899520	-0.109966	4.046187
572.754452	5609.687250	7.904525	-0.109985	4.049017
572.832508	5617.742423	7.909530	-0.110005	4.051854
573.405115	5625.698641	7.914534	-0.110117	4.054661
573.411687	5633.787816	7.919539	-0.110123	4.057504
573.857310	5641.736896	7.924544	-0.110211	4.060303
574.178702	5649.775205	7.929549	-0.110277	4.063129
574.790720	5657.774092	7.934554	-0.110396	4.065943
575.199703	5665.772131	7.939558	-0.110477	4.068752
575.313707	5673.871086	7.944563	-0.110504	4.071590
575.340032	5681.870516	7.949568	-0.110514	4.074391
575.890718	5689.892240	7.954573	-0.110621	4.077204
576.179069	5697.879577	7.959578	-0.110680	4.080000
576.182799	5705.897560	7.964582	-0.110686	4.082800
576.683416	5713.942913	7.969587	-0.110785	4.085615
576.100529	5722.016376	7.974592	-0.110681	4.088423
576.589392	5730.021537	7.979597	-0.110778	4.091220
577.223679	5737.960210	7.984602	-0.110901	4.093994
577.234230	5746.035285	7.989606	-0.110908	4.096805
577.945835	5753.994724	7.994611	-0.111046	4.099583
578.134495	5762.036219	7.999616	-0.111086	4.102381
578.139520	5770.073419	8.004621	-0.111092	4.105172
578.537360	5778.111544	8.009626	-0.111172	4.107968
579.129842	5786.108133	8.014630	-0.111287	4.110749
579.562000	5794.116597	8.019635	-0.111373	4.113531
579.677675	5802.157278	8.024640	-0.111400	4.116318
579.937982	5810.103189	8.029645	-0.111453	4.119072
580.438254	5818.187138	8.034650	-0.111552	4.121875
580.471265	5826.132797	8.039654	-0.111563	4.124622
581.035263	5834.228293	8.044659	-0.111673	4.127426
581.148314	5842.255078	8.049664	-0.111700	4.130198
581.450883	5850.282050	8.054669	-0.111761	4.132971
581.668768	5858.282358	8.059674	-0.111807	4.135732
582.100579	5866.210407	8.064678	-0.111893	4.138468
582.442557	5874.340414	8.069683	-0.111962	4.141272
582.384619	5882.282808	8.074688	-0.111956	4.144003
582.714643	5890.339869	8.079693	-0.112023	4.146778
583.530484	5898.338556	8.084698	-0.112180	4.149536
583.583881	5906.403060	8.089702	-0.112195	4.152305
584.225215	5914.379147	8.094707	-0.112320	4.155050
584.372530	5922.392003	8.099712	-0.112352	4.157799
584.829724	5930.418418	8.104717	-0.112443	4.160555
585.010387	5938.424502	8.109722	-0.112482	4.163299
585.349980	5946.472376	8.114726	-0.112550	4.166057
585.800145	5954.500884	8.119731	-0.112639	4.168807
585.725237	5962.606042	8.124736	-0.112630	4.171576
586.168161	5970.547875	8.129741	-0.112718	4.174294
586.574456	5978.595154	8.134746	-0.112799	4.177045
586.903070	5986.576382	8.139750	-0.112865	4.179771
587.302549	5994.610050	8.144755	-0.112945	4.182513
587.421934	6002.623727	8.149760	-0.112972	4.185244
587.822676	6010.625962	8.154765	-0.113052	4.187972
587.954185	6018.708629	8.159770	-0.113082	4.190723
588.220755	6026.721469	8.164774	-0.113137	4.193450
588.924176	6034.758414	8.169779	-0.113273	4.196188
588.852788	6042.711168	8.174784	-0.113265	4.198887
589.093791	6050.738062	8.179789	-0.113315	4.201613
589.631008	6058.700860	8.184794	-0.113420	4.204318
590.365206	6066.717095	8.189798	-0.113562	4.207042
590.481957	6074.794452	8.194803	-0.113589	4.209778
590.587959	6082.844231	8.199808	-0.113614	4.212503
591.283709	6090.797623	8.204813	-0.113749	4.215200
591.499004	6098.834247	8.209818	-0.113794	4.217918
591.541510	6106.881512	8.214822	-0.113808	4.220636
592.046288	6114.845707	8.219827	-0.113907	4.223329
592.094708	6122.909740	8.224832	-0.113921	4.226049
592.622087	6130.883805	8.229837	-0.114024	4.228742
592.942822	6138.960291	8.234842	-0.114089	4.231466
592.906086	6146.922970	8.239846	-0.114088	4.234146
593.258241	6155.019263	8.244851	-0.114159	4.236873
593.792598	6162.915791	8.249856	-0.114263	4.239533
594.557496	6170.918545	8.254861	-0.114411	4.242229
594.585649	6179.009659	8.259866	-0.114421	4.244946
594.651953	6187.008996	8.264870	-0.114439	4.247630
595.158122	6195.039849	8.269875	-0.114538	4.250328
595.366682	6203.099464	8.274880	-0.114582	4.253031
595.869038	6211.082261	8.279885	-0.114681	4.255709
596.022569	6219.145484	8.284890	-0.114715	4.258409
596.476530	6227.092473	8.289894	-0.114805	4.261071
596.740602	6235.100374	8.294899	-0.114859	4.263750
596.774615	6243.178699	8.299904	-0.114871	4.266449
597.058810	6251.126177	8.304909	-0.114929	4.269104
597.392836	6259.282382	8.309914	-0.114996	4.271828
597.901261	6267.162872	8.314918	-0.115096	4.274460
597.748708	6275.310858	8.319923	-0.115073	4.277173
598.234836	6283.214299	8.324928	-0.115169	4.279809
598.551783	6291.235232	8.329933	-0.115233	4.282481
598.980517	6299.248979	8.334938	-0.115318	4.285150
599.144109	6307.237240	8.339942	-0.115354	4.287806
599.433330	6315.320361	8.344947	-0.115413	4.290493
599.935966	6323.297806	8.349952	-0.115512	4.293145
600.321576	6331.386948	8.354957	-0.115589	4.295832
600.357646	6339.401616	8.359962	-0.115601	4.298489
600.831947	6347.420621	8.364966	-0.115694	4.301149
601.010649	6355.388021	8.369971	-0.115733	4.303789
601.454168	6363.429348	8.374976	-0.115821	4.306453
601.771865	6371.400542	8.379981	-0.115885	4.309091
601.837964	6379.488727	8.384986	-0.115902	4.311765
602.210161	6387.412874	8.389990	-0.115977	4.314385
602.587781	6395.509343	8.394995	-0.116052	4.317060
602.755548	6403.412420	8.400000	-0.116089	4.319668
603.221983	6411.478154	8.405005	-0.116181	4.322331
603.519140	6419.524575	8.410010	-0.116242	4.324984
603.354380	6427.552620	8.415014	-0.116216	4.327626
603.965720	6435.535410	8.420019	-0.116335	4.330257
604.390963	6443.543696	8.425024	-0.116420	4.332893
604.579864	6451.606090	8.430029	-0.116460	4.335544
605.053296	6459.573946	8.435034	-0.116553	4.338165
605.309905	6467.678177	8.440038	-0.116606	4.340826
605.477846	6475.651393	8.445043	-0.116643	4.343443
605.482026	6483.660688	8.450048	-0.116649	4.346068
605.990553	6491.676335	8.455053	-0.116749	4.348698
606.266841	6499.742078	8.460058	-0.116805	4.351341
606.881301	6507.701644	8.465062	-0.116925	4.353950
606.812213	6515.850587	8.470067	-0.116918	4.356614
607.174777	6523.712664	8.475072	-0.116990	4.359186
607.414547	6531.762780	8.480077	-0.117040	4.361817
607.502540	6539.793215	8.485082	-0.117062	4.364439
607.496582	6547.824678	8.490086	-0.117066	4.367059
608.390609	6555.760566	8.495091	-0.117237	4.369652
608.234546	6563.878591	8.500096	-0.117214	4.372296
608.451868	6571.904952	8.505101	-0.117259	4.374911
609.124393	6579.921605	8.510106	-0.117390	4.377524
609.286189	6587.884018	8.515110	-0.117425	4.380115
609.485674	6595.946579	8.520115	-0.117468	4.382736
609.906016	6603.932983	8.525120	-0.117551	4.385333
610.248190	6611.946919	8.530125	-0.117620	4.387937
610.169691	6620.060152	8.535130	-0.117611	4.390569
610.196841	6628.033760	8.540134	-0.117621	4.393155
610.737361	6636.085686	8.545139	-0.117727	4.395767
611.202209	6644.035983	8.550144	-0.117819	4.398345
611.481320	6652.103447	8.555149	-0.117876	4.400957
612.081961	6660.029255	8.560154	-0.117993	4.403525
612.468694	6668.066994	8.565159	-0.118070	4.406125
612.447044	6676.150451	8.570163	-0.118071	4.408737
613.057859	6684.148715	8.575168	-0.118190	4.411323
613.293190	6692.179481	8.580173	-0.118239	4.413916
613.755536	6700.260713	8.585178	-0.118331	4.416524
613.887003	6708.190501	8.590183	-0.118360	4.419081
614.728586	6716.229848	8.595187	-0.118522	4.421675
614.779645	6724.258698	8.600192	-0.118537	4.424260
615.212081	6732.277549	8.605197	-0.118623	4.426842
615.508453	6740.323767	8.610202	-0.118683	4.429431
615.889753	6748.326874	8.615207	-0.118759	4.432005
616.114414	6756.337161	8.620211	-0.118806	4.434579
616.195983	6764.421463	8.625216	-0.118827	4.437174
616.603871	6772.373343	8.630221	-0.118908	4.439727
616.966871	6780.380298	8.635226	-0.118981	4.442295
617.076274	6788.326474	8.640231	-0.119006	4.444842
617.345828	6796.430052	8.645235	-0.119062	4.447438
617.228440	6804.441416	8.650240	-0.119045	4.450002
617.591088	6812.474198	8.655245	-0.119118	4.452573
618.201551	6820.483021	8.660250	-0.119237	4.455136
618.844415	6828.411234	8.665255	-0.119362	4.457671
619.054220	6836.504450	8.670259	-0.119406	4.460256
619.467390	6844.458897	8.675264	-0.119488	4.462796
620.022785	6852.497509	8.680269	-0.119597	4.465362
620.206264	6860.567198	8.685274	-0.119636	4.467935
620.520687	6868.545889	8.690279	-0.119700	4.470478
620.624345	6876.651489	8.695283	-0.119725	4.473059
620.691494	6884.604239	8.700288	-0.119742	4.475590
620.871406	6892.540556	8.705293	-0.119781	4.478114
621.508021	6900.622552	8.710298	-0.119905	4.480685
621.779872	6908.548428	8.715303	-0.119961	4.483204
621.845229	6916.683835	8.720307	-0.119978	4.485787
622.136751	6924.618713	8.725312	-0.120037	4.488305
622.914862	6932.633681	8.730317	-0.120188	4.490849
623.278892	6940.675636	8.735322	-0.120261	4.493399
622.959727	6948.731383	8.740327	-0.120206	4.495949
623.647997	6956.680682	8.745331	-0.120340	4.498468
623.386391	6964.788337	8.750336	-0.120296	4.501032
624.122347	6972.661594	8.755341	-0.120439	4.503524
624.407505	6980.782998	8.760346	-0.120497	4.506091
624.918530	6988.743873	8.765351	-0.120597	4.508607
625.056907	6996.855311	8.770355	-0.120628	4.511167
625.578804	7004.793730	8.775360	-0.120731	4.513673
625.865640	7012.869597	8.780365	-0.120789	4.516220
625.636699	7020.896117	8.785370	-0.120752	4.518748
625.972419	7028.852877	8.790375	-0.120820	4.521255
626.265191	7036.804624	8.795379	-0.120879	4.523759
626.812057	7044.884936	8.800384	-0.120986	4.526302
627.168010	7052.824504	8.805389	-0.121058	4.528799
627.503011	7060.941697	8.810394	-0.121126	4.531350
628.022277	7068.883233	8.815399	-0.121227	4.533845
628.201620	7076.982067	8.820403	-0.121266	4.536387
628.236575	7084.911321	8.825408	-0.121278	4.538875
628.446193	7093.028030	8.830413	-0.121322	4.541420
629.099527	7100.944101	8.835418	-0.121449	4.543901
629.223703	7108.980873	8.840423	-0.121477	4.546418
629.455220	7117.008511	8.845427	-0.121526	4.548931
629.838549	7125.105659	8.850432	-0.121602	4.551465
630.175563	7133.021950	8.855437	-0.121670	4.553940
630.365153	7141.157413	8.860442	-0.121711	4.556482
630.534638	7149.063604	8.865447	-0.121747	4.558952
630.473364	7157.150477	8.870451	-0.121741	4.561475
630.781732	7165.062728	8.875456	-0.121804	4.563944
630.606756	7173.225169	8.880461	-0.121777	4.566488
631.359406	7181.119140	8.885466	-0.121922	4.568949
631.322414	7189.229807	8.890471	-0.121920	4.571475
631.729957	7197.145377	8.895475	-0.122001	4.573939
631.991327	7205.221590	8.900480	-0.122055	4.576452
632.239628	7213.139680	8.905485	-0.122107	4.578914
632.609452	7221.292839	8.910490	-0.122181	4.581448
632.821307	7229.144519	8.915495	-0.122225	4.583886
632.880822	7237.347084	8.920499	-0.122242	4.586432
633.073388	7245.260876	8.925504	-0.122283	4.588887
633.269202	7253.369346	8.930509	-0.122325	4.591401
633.693488	7261.336599	8.935514	-0.122409	4.593871
633.685748	7269.383018	8.940519	-0.122413	4.596363
634.195086	7277.272183	8.945523	-0.122513	4.598805
634.676059	7285.301074	8.950528	-0.122607	4.601289
634.516405	7293.292322	8.955533	-0.122583	4.603760
635.135887	7301.344040	8.960538	-0.122704	4.606248
635.108287	7309.376095	8.965543	-0.122704	4.608729
636.095221	7317.369616	8.970547	-0.122893	4.611197
636.048481	7325.391287	8.975552	-0.122889	4.613672
635.747260	7333.514724	8.980557	-0.122838	4.616177
635.893242	7341.504310	8.985562	-0.122871	4.618639
636.469252	7349.506087	8.990567	-0.122983	4.621104
636.965768	7357.450522	8.995571	-0.123081	4.623550
637.720870	7365.482544	9.000576	-0.123227	4.626021
638.079608	7373.434872	9.005581	-0.123299	4.628466
638.639621	7381.546039	9.010586	-0.123408	4.630959
639.057267	7389.509253	9.015591	-0.123491	4.633405
639.420449	7397.554118	9.020595	-0.123564	4.635875
639.822090	7405.479293	9.025600	-0.123644	4.638307
640.079723	7413.560367	9.030605	-0.123697	4.640785
640.597239	7421.583016	9.035610	-0.123799	4.643244
640.509066	7429.630688	9.040615	-0.123788	4.645710
640.832167	7437.659806	9.045619	-0.123853	4.648168
641.217021	7445.650560	9.050624	-0.123930	4.650613
641.257243	7453.676644	9.055629	-0.123943	4.653068
641.286583	7461.758044	9.060634	-0.123953	4.655538
641.528091	7469.715477	9.065639	-0.124004	4.657969
642.210770	7477.690576	9.070643	-0.124136	4.660404
641.970060	7485.741229	9.075648	-0.124096	4.662862
642.862810	7493.682702	9.080653	-0.124268	4.665283
643.179287	7501.808131	9.085658	-0.124332	4.667760
643.424938	7509.764574	9.090663	-0.124383	4.670185
643.572510	7517.883837	9.095667	-0.124416	4.672657
644.223947	7525.862654	9.100672	-0.124542	4.675085
643.931796	7533.939663	9.105677	-0.124493	4.677543
644.721388	7541.833255	9.110682	-0.124645	4.679942
644.769551	7549.910890	9.115687	-0.124659	4.682397
645.115416	7557.888251	9.120691	-0.124729	4.684820
644.832555	7565.975938	9.125696	-0.124682	4.687275
645.024869	7573.946610	9.130701	-0.124723	4.689694
645.504765	7581.983706	9.135706	-0.124817	4.692130
645.987880	7589.909805	9.140711	-0.124912	4.694532
646.210247	7598.006735	9.145715	-0.124959	4.696985
646.784637	7605.902709	9.150720	-0.125071	4.699375
646.945756	7613.998604	9.155725	-0.125106	4.701824
646.764054	7622.061595	9.160730	-0.125078	4.704264
647.424662	7630.010070	9.165735	-0.125206	4.706665
648.169984	7638.006826	9.170739	-0.125350	4.709080
648.340588	7646.102365	9.175744	-0.125387	4.711525
648.491546	7654.032378	9.180749	-0.125420	4.713918
648.989893	7662.187360	9.185754	-0.125518	4.716377
649.333384	7670.049474	9.190759	-0.125587	4.718747
649.672750	7678.162261	9.195763	-0.125656	4.721192
649.849049	7686.127812	9.200768	-0.125694	4.723590
650.129772	7694.168846	9.205773	-0.125752	4.726011
650.489426	7702.158715	9.210778	-0.125824	4.728414
650.972452	7710.184969	9.215783	-0.125919	4.730827
651.214970	7718.258148	9.220787	-0.125969	4.733253
651.386668	7726.295460	9.225792	-0.126006	4.735667
651.391317	7734.260588	9.230797	-0.126013	4.738059
651.517361	7742.407735	9.235802	-0.126041	4.740504
651.616743	7750.327789	9.240807	-0.126065	4.742879
652.132514	7758.309958	9.245811	-0.126166	4.745271
651.981518	7766.402471	9.250816	-0.126143	4.747696
652.291322	7774.398305	9.255821	-0.126206	4.750090
652.655730	7782.407194	9.260826	-0.126279	4.752487
652.708885	7790.435873	9.265831	-0.126294	4.754889
652.925356	7798.435885	9.270835	-0.126340	4.757281
653.218824	7806.383372	9.275840	-0.126400	4.759655
653.710275	7814.397719	9.280845	-0.126497	4.762048
654.183312	7822.343930	9.285850	-0.126590	4.764419
654.529188	7830.407961	9.290855	-0.126659	4.766825
655.131114	7838.385959	9.295859	-0.126777	4.769202
655.233263	7846.518439	9.300864	-0.126801	4.771627
655.497876	7854.431708	9.305869	-0.126856	4.773984
655.730410	7862.572991	9.310874	-0.126904	4.776408
656.378278	7870.448732	9.315879	-0.127030	4.778750
656.887976	7878.504255	9.320883	-0.127130	4.781145
656.610888	7886.559355	9.325888	-0.127084	4.783541
656.631196	7894.601190	9.330893	-0.127093	4.785931
657.119908	7902.604795	9.335898	-0.127189	4.788307
657.605308	7910.611477	9.340903	-0.127285	4.790683
657.747278	7918.609310	9.345907	-0.127316	4.793056
658.022862	7926.666676	9.350912	-0.127373	4.795445
658.345578	7934.596110	9.355917	-0.127438	4.797794
658.478161	7942.746097	9.360922	-0.127468	4.800209
658.920520	7950.654759	9.365927	-0.127556	4.802549
659.329082	7958.653469	9.370931	-0.127637	4.804916
659.381377	7966.762968	9.375936	-0.127652	4.807315
659.530673	7974.688969	9.380941	-0.127685	4.809658
659.917348	7982.788313	9.385946	-0.127762	4.812051
660.313994	7990.194396	9.390951	-0.127841	4.814237
660.565816	7994.980592	9.395955	-0.127891	4.815649

661.061442	7997.535349	9.400960	-0.127985	4.816401
661.230227	7998.845000	9.405965	-0.128017	4.816787
661.346334	7999.396713	9.410970	-0.128039	4.816950
661.114084	8000.479302	9.415975	-0.127996	4.817270
661.476586	8000.499693	9.420979	-0.128064	4.817275
661.667612	8000.469849	9.425984	-0.128100	4.817265
661.732464	8000.470848	9.430989	-0.128112	4.817265
662.129874	8000.472741	9.435994	-0.128186	4.817264
662.172670	8000.427921	9.440999	-0.128194	4.817250
662.473247	8000.475917	9.446003	-0.128250	4.817263
662.703577	8000.474179	9.451008	-0.128292	4.817261
662.927693	8000.511480	9.456013	-0.128334	4.817271
662.894307	8000.435870	9.461018	-0.128328	4.817249
662.481007	8000.476038	9.466023	-0.128251	4.817263
662.856492	8000.529421	9.471027	-0.128321	4.817277
663.090614	8000.447357	9.476032	-0.128365	4.817252
663.479773	8000.471338	9.481037	-0.128437	4.817257
663.580860	8000.508858	9.486042	-0.128456	4.817268
663.886658	8000.442708	9.491047	-0.128513	4.817247
664.359514	8000.416153	9.496051	-0.128601	4.817237
664.490634	8000.346251	9.501056	-0.128625	4.817216
664.107315	8000.503227	9.506061	-0.128554	4.817264
664.266874	8000.541651	9.511066	-0.128584	4.817274
664.546261	8000.490959	9.516071	-0.128636	4.817258
664.620706	8000.430760	9.521075	-0.128649	4.817240
664.727844	8000.536070	9.526080	-0.128669	4.817271
664.562134	8000.466877	9.531085	-0.128639	4.817251
664.485384	8000.460405	9.536090	-0.128624	4.817249
664.737774	8000.518242	9.541095	-0.128671	4.817265
664.455975	8000.472644	9.546099	-0.128619	4.817253
664.548465	8000.466667	9.551104	-0.128636	4.817251
664.818659	8000.557569	9.556109	-0.128686	4.817276
664.936467	8000.398612	9.561114	-0.128708	4.817229
664.861853	8000.470444	9.566119	-0.128694	4.817251
664.847084	8000.540027	9.571123	-0.128692	4.817271
665.018924	8000.452771	9.576128	-0.128724	4.817245
665.000556	8000.457776	9.581133	-0.128720	4.817246
665.166772	8000.375722	9.586138	-0.128751	4.817221
665.462547	8000.508273	9.591143	-0.128806	4.817259
665.631398	8000.451645	9.596147	-0.128838	4.817241
665.531330	8000.565395	9.601152	-0.128819	4.817276
666.139385	8000.444677	9.606157	-0.128932	4.817237
666.221053	8000.401511	9.611162	-0.128947	4.817224
665.723598	8000.458357	9.616167	-0.128855	4.817243
665.919733	8000.540716	9.621171	-0.128891	4.817266
665.588474	8000.479543	9.626176	-0.128830	4.817250
665.607688	8000.495706	9.631181	-0.128833	4.817255
665.287776	8000.321531	9.636186	-0.128774	4.817205
665.350634	8000.443083	9.641191	-0.128785	4.817240
665.554881	8000.288631	9.646195	-0.128823	4.817194
665.832703	8000.415616	9.651200	-0.128875	4.817230
665.600063	8000.232211	9.656205	-0.128832	4.817177
665.883607	8000.341302	9.661210	-0.128885	4.817208
666.091810	8000.478851	9.666215	-0.128923	4.817247
666.223955	8000.490411	9.671219	-0.128948	4.817250
666.161905	8000.400601	9.676224	-0.128936	4.817224
666.336248	8000.481567	9.681229	-0.128969	4.817247
666.597440	8000.434826	9.686234	-0.129018	4.817232
666.217470	8000.473387	9.691239	-0.128947	4.817245
666.377270	8000.353153	9.696243	-0.128977	4.817209
666.652229	8000.460001	9.701248	-0.129028	4.817239
666.543484	8000.447745	9.706253	-0.129008	4.817236
667.338436	8000.537239	9.711258	-0.129156	4.817259
667.285337	8000.509974	9.716263	-0.129146	4.817251
666.793454	8000.471703	9.721267	-0.129054	4.817242
666.814811	8000.459339	9.726272	-0.129058	4.817238
667.695204	8000.389370	9.731277	-0.129222	4.817214
668.065971	8000.458565	9.736282	-0.129291	4.817232
667.325856	8000.473578	9.741287	-0.129153	4.817240
667.383837	8000.491399	9.746291	-0.129164	4.817245
667.288597	8000.528008	9.751296	-0.129146	4.817256
666.934718	8000.432632	9.756301	-0.129080	4.817230
667.317361	8000.536915	9.761306	-0.129152	4.817259
666.873948	8000.348129	9.766311	-0.129069	4.817205
667.086757	8000.352473	9.771315	-0.129109	4.817206
666.952486	8000.357804	9.776320	-0.129084	4.817208
667.543176	8000.527711	9.781325	-0.129194	4.817255
667.674128	8000.475786	9.786330	-0.129218	4.817239
667.558668	8000.525835	9.791335	-0.129197	4.817255
667.335168	8000.545654	9.796339	-0.129155	4.817261
667.687310	8000.546863	9.801344	-0.129221	4.817260
667.453844	8000.479789	9.806349	-0.129177	4.817241
667.625387	8000.552253	9.811354	-0.129209	4.817262
667.789643	8000.401409	9.816359	-0.129240	4.817217
667.247708	8000.426889	9.821363	-0.129139	4.817227
667.086904	8000.452967	9.826368	-0.129109	4.817235
667.223721	8000.402190	9.831373	-0.129134	4.817220
667.340643	8000.361684	9.836378	-0.129156	4.817207
667.337421	8000.575309	9.841383	-0.129156	4.817270
667.781866	8000.477452	9.846387	-0.129238	4.817239
667.646625	8000.565277	9.851392	-0.129213	4.817266
667.550808	8000.467537	9.856397	-0.129195	4.817237
667.583249	8000.327351	9.861402	-0.129201	4.817196
667.943264	8000.519085	9.866407	-0.129268	4.817251
668.113073	8000.443431	9.871411	-0.129300	4.817228
667.782443	8000.472173	9.876416	-0.129238	4.817238
667.500792	8000.384257	9.881421	-0.129186	4.817213
667.406421	8000.142684	9.886426	-0.129168	4.817142
667.818899	8000.450523	9.891431	-0.129245	4.817231
668.506666	8000.489710	9.896435	-0.129373	4.817240
668.557600	8000.500018	9.901440	-0.129383	4.817242
668.214673	8000.464042	9.906445	-0.129319	4.817233
668.105866	8000.469766	9.911450	-0.129299	4.817236
668.100277	8000.551132	9.916455	-0.129298	4.817260
668.151192	8000.447195	9.921459	-0.129307	4.817229
668.021627	8000.500200	9.926464	-0.129283	4.817245
668.509191	8000.463305	9.931469	-0.129374	4.817232
668.291850	8000.474756	9.936474	-0.129333	4.817236
668.723942	8000.478260	9.941479	-0.129414	4.817235
668.254302	8000.492159	9.946483	-0.129326	4.817241
668.481152	8000.481913	9.951488	-0.129368	4.817237
668.308888	8000.488772	9.956493	-0.129336	4.817240
668.719437	8000.464439	9.961498	-0.129413	4.817231
668.832285	8000.569851	9.966503	-0.129434	4.817262
668.997046	8000.499407	9.971507	-0.129465	4.817240
669.342648	8000.452915	9.976512	-0.129529	4.817225
668.779548	8000.537301	9.981517	-0.129424	4.817252
668.831128	8000.512711	9.986522	-0.129434	4.817245
668.615580	8000.431101	9.991527	-0.129393	4.817222
669.215008	8000.484794	9.996531	-0.129505	4.817235
668.857436	8000.516291	10.001536	-0.129439	4.817246
669.222641	8000.453177	10.006541	-0.129507	4.817226
669.004764	8000.542899	10.011546	-0.129466	4.817253
668.884040	8000.435250	10.016551	-0.129443	4.817222
669.033231	8000.531703	10.021555	-0.129471	4.817250
669.038490	8000.463025	10.026560	-0.129472	4.817229
668.881182	8000.493387	10.031565	-0.129443	4.817239
668.755173	8000.563372	10.036570	-0.129420	4.817260
668.752342	8000.440620	10.041575	-0.129419	4.817224
668.977138	8000.448326	10.046579	-0.129461	4.817225
669.327674	8000.444224	10.051584	-0.129526	4.817222
669.023526	8000.511456	10.056589	-0.129470	4.817244
668.974001	8000.466261	10.061594	-0.129460	4.817231
669.646293	8000.420588	10.066599	-0.129585	4.817214
669.899938	8000.419220	10.071603	-0.129633	4.817212
669.808134	8000.447420	10.076608	-0.129616	4.817221
670.128386	8000.323314	10.081613	-0.129675	4.817183
670.424620	8000.339531	10.086618	-0.129730	4.817187
669.935095	8000.376392	10.091623	-0.129639	4.817200
670.036811	8000.413932	10.096627	-0.129658	4.817210
669.891882	8000.515361	10.101632	-0.129631	4.817241
670.008035	8000.439934	10.106637	-0.129653	4.817218
669.788621	8000.534922	10.111642	-0.129612	4.817247
669.745340	8000.457030	10.116647	-0.129604	4.817224
669.912881	8000.385570	10.121651	-0.129635	4.817202
669.894518	8000.523866	10.126656	-0.129632	4.817243
669.931763	8000.463086	10.131661	-0.129639	4.817225
669.982680	8000.523114	10.136666	-0.129648	4.817243
669.895559	8000.500609	10.141671	-0.129632	4.817236
670.133620	8000.475729	10.146675	-0.129676	4.817228
669.999837	8000.506454	10.151680	-0.129651	4.817238
669.550579	8000.415938	10.156685	-0.129568	4.817213
669.847115	8000.480820	10.161690	-0.129623	4.817231
669.861163	8000.460938	10.166695	-0.129626	4.817225
669.863509	8000.580512	10.171699	-0.129626	4.817260
669.630543	8000.475356	10.176704	-0.129583	4.817230
669.834369	8000.471103	10.181709	-0.129621	4.817228
670.029808	8000.438158	10.186714	-0.129657	4.817217
669.881832	8000.541656	10.191719	-0.129629	4.817249
669.944279	8000.481266	10.196723	-0.129641	4.817231
670.183149	8000.479670	10.201728	-0.129686	4.817229
670.217035	8000.435764	10.206733	-0.129692	4.817216
670.102796	8000.511222	10.211738	-0.129671	4.817239
670.157783	8000.516304	10.216743	-0.129681	4.817240
670.194430	8000.461862	10.221747	-0.129688	4.817224
669.631226	8000.546245	10.226752	-0.129583	4.817251
669.412760	8000.489975	10.231757	-0.129542	4.817236
669.627296	8000.479540	10.236762	-0.129582	4.817231
669.835222	8000.516606	10.241767	-0.129621	4.817241
670.114608	8000.526216	10.246771	-0.129673	4.817243
670.090432	8000.453907	10.251776	-0.129668	4.817222
669.858921	8000.427055	10.256781	-0.129625	4.817215
670.369050	8000.530151	10.261786	-0.129720	4.817243
670.531729	8000.455443	10.266791	-0.129750	4.817220
670.756843	8000.476909	10.271795	-0.129792	4.817226
670.701358	8000.487687	10.276800	-0.129782	4.817229
670.143143	8000.508675	10.281805	-0.129678	4.817238
670.212798	8000.454743	10.286810	-0.129691	4.817221
670.084297	8000.518344	10.291815	-0.129667	4.817241
670.015767	8000.468622	10.296819	-0.129654	4.817226
670.238268	8000.548230	10.301824	-0.129696	4.817249
670.520482	8000.438344	10.306829	-0.129748	4.817215
670.389278	8000.480746	10.311834	-0.129724	4.817228
670.297812	8000.457117	10.316839	-0.129707	4.817222
669.705451	8000.353809	10.321843	-0.129597	4.817194
669.933526	8000.412343	10.326848	-0.129639	4.817210
670.142170	8000.528761	10.331853	-0.129678	4.817244
670.371138	8000.451904	10.336858	-0.129721	4.817220
670.815926	8000.420700	10.341863	-0.129803	4.817209
670.755727	8000.475836	10.346867	-0.129792	4.817225
670.829106	8000.510824	10.351872	-0.129806	4.817235
670.820474	8000.488475	10.356877	-0.129804	4.817229
671.141761	8000.502966	10.361882	-0.129864	4.817231
670.505899	8000.447642	10.366887	-0.129746	4.817218
671.064357	8000.440412	10.371891	-0.129850	4.817213
670.872677	8000.530541	10.376896	-0.129814	4.817241
670.729935	8000.486017	10.381901	-0.129787	4.817228
670.594863	8000.465945	10.386906	-0.129762	4.817223
670.672091	8000.463966	10.391911	-0.129777	4.817222
670.595115	8000.522016	10.396915	-0.129762	4.817240
670.898408	8000.452656	10.401920	-0.129819	4.817218
670.704019	8000.553322	10.406925	-0.129783	4.817248
670.718587	8000.534505	10.411930	-0.129785	4.817243
671.028086	8000.398595	10.416935	-0.129843	4.817201
670.955903	8000.524425	10.421939	-0.129830	4.817239
671.493019	8000.461856	10.426944	-0.129929	4.817218
671.393046	8000.323842	10.431949	-0.129911	4.817177
671.513092	8000.438893	10.436954	-0.129933	4.817211
671.494640	8000.407929	10.441959	-0.129930	4.817202
671.450090	8000.408298	10.446963	-0.129921	4.817202
671.147709	8000.494598	10.451968	-0.129865	4.817229
671.379589	8000.409323	10.456973	-0.129908	4.817203
671.218894	8000.449153	10.461978	-0.129878	4.817215
671.112300	8000.481357	10.466983	-0.129859	4.817225
671.323022	8000.438070	10.471987	-0.129898	4.817212
671.516795	8000.506657	10.476992	-0.129934	4.817231
671.493929	8000.419556	10.481997	-0.129930	4.817205
671.403673	8000.439318	10.487002	-0.129913	4.817212
671.540123	8000.478456	10.492007	-0.129938	4.817222
671.317798	8000.521563	10.497011	-0.129897	4.817236
671.575273	8000.444089	10.502016	-0.129945	4.817212
671.456651	8000.409459	10.507021	-0.129923	4.817202
671.885033	8000.394930	10.512026	-0.130002	4.817196
671.483343	8000.456420	10.517031	-0.129928	4.817216
671.298604	8000.509630	10.522035	-0.129893	4.817233
671.496050	8000.412185	10.527040	-0.129930	4.817203
671.054520	8000.523838	10.532045	-0.129848	4.817238
670.900671	8000.493953	10.537050	-0.129819	4.817230
670.911894	8000.487780	10.542055	-0.129821	4.817228
671.091973	8000.456714	10.547059	-0.129855	4.817218
671.285810	8000.536939	10.552064	-0.129891	4.817241
671.623962	8000.418397	10.557069	-0.129954	4.817204
671.600186	8000.501603	10.562074	-0.129950	4.817229
670.927503	8000.442533	10.567079	-0.129824	4.817215
670.652032	8000.475298	10.572083	-0.129773	4.817226
671.037228	8000.404032	10.577088	-0.129845	4.817203
670.628715	8000.468591	10.582093	-0.129769	4.817224
671.152313	8000.376191	10.587098	-0.129866	4.817194
670.932933	8000.506091	10.592103	-0.129825	4.817233
671.253464	8000.451809	10.597107	-0.129885	4.817216
671.035733	8000.515087	10.602112	-0.129844	4.817236
671.373853	8000.450498	10.607117	-0.129907	4.817215
671.444088	8000.485437	10.612122	-0.129920	4.817225
671.016963	8000.508450	10.617127	-0.129841	4.817234
670.783443	8000.411745	10.622131	-0.129797	4.817206
671.420483	8000.482957	10.627136	-0.129916	4.817224
671.100558	8000.566870	10.632141	-0.129857	4.817251
671.091474	8000.359384	10.637146	-0.129855	4.817189
670.950206	8000.492608	10.642151	-0.129829	4.817229
671.068125	8000.481738	10.647155	-0.129850	4.817226
670.870144	8000.410971	10.652160	-0.129814	4.817206
670.574483	8000.358794	10.657165	-0.129758	4.817192
670.841157	8000.377729	10.662170	-0.129808	4.817196
670.909700	8000.506792	10.667175	-0.129821	4.817234
671.068016	8000.451058	10.672179	-0.129850	4.817217
671.527232	8000.444410	10.677184	-0.129936	4.817212
671.102043	8000.498132	10.682189	-0.129857	4.817230
671.067190	8000.422483	10.687194	-0.129850	4.817208
670.906902	8000.226413	10.692199	-0.129820	4.817151
671.412186	8000.486005	10.697203	-0.129915	4.817225
670.898080	8000.524598	10.702208	-0.129819	4.817239
671.111235	8000.489812	10.707213	-0.129859	4.817228
671.523252	8000.495129	10.712218	-0.129935	4.817227
670.849064	8000.402184	10.717223	-0.129810	4.817203
671.081517	8000.437516	10.722227	-0.129853	4.817212
671.017422	8000.483072	10.727232	-0.129841	4.817226
670.856076	8000.529239	10.732237	-0.129811	4.817241
671.049722	8000.304790	10.737242	-0.129847	4.817173
671.117923	8000.576664	10.742247	-0.129860	4.817253
671.028396	8000.373223	10.747251	-0.129843	4.817194
671.059957	8000.514410	10.752256	-0.129849	4.817235
671.075925	8000.424736	10.757261	-0.129852	4.817209
671.264284	8000.228769	10.762266	-0.129887	4.817150
670.854225	8000.465738	10.767271	-0.129811	4.817222
670.773688	8000.268787	10.772275	-0.129796	4.817164
670.832688	8000.309898	10.777280	-0.129807	4.817176
670.607626	8000.386816	10.782285	-0.129765	4.817200
670.564136	8000.219001	10.787290	-0.129757	4.817150
670.706867	8000.409509	10.792295	-0.129783	4.817206
670.663524	8000.379218	10.797299	-0.129775	4.817197
670.897582	8000.494973	10.802304	-0.129819	4.817230
670.941477	8000.405733	10.807309	-0.129827	4.817204
671.456368	8000.390424	10.812314	-0.129923	4.817197
670.977976	8000.405240	10.817319	-0.129834	4.817203
670.889321	8000.297023	10.822323	-0.129817	4.817172
671.272682	8000.300837	10.827328	-0.129889	4.817171
671.105034	8000.246408	10.832333	-0.129857	4.817156
671.066775	8000.155898	10.837338	-0.129850	4.817129
670.742026	8000.225985	10.842343	-0.129790	4.817152
671.015384	8000.266180	10.847347	-0.129841	4.817162
671.245606	8000.370239	10.852352	-0.129884	4.817192
671.059253	8000.510171	10.857357	-0.129849	4.817234
671.215102	8000.411025	10.862362	-0.129878	4.817204
670.754208	8000.411301	10.867367	-0.129792	4.817206
670.677933	8000.209127	10.872371	-0.129778	4.817147
671.445444	8000.563752	10.877376	-0.129921	4.817248
671.257713	8000.468811	10.882381	-0.129886	4.817221
671.004869	8000.219472	10.887386	-0.129839	4.817148
671.132866	8000.488037	10.892391	-0.129863	4.817227
671.195394	8000.404374	10.897395	-0.129874	4.817202
671.356285	8000.421674	10.902400	-0.129904	4.817207
671.177628	8000.413621	10.907405	-0.129871	4.817205
671.264377	8000.221371	10.912410	-0.129887	4.817148
671.419209	8000.457558	10.917415	-0.129916	4.817217
671.452810	8000.495104	10.922419	-0.129922	4.817228
671.124871	8000.263644	10.927424	-0.129861	4.817161
671.240208	8000.361695	10.932429	-0.129883	4.817189
670.767328	8000.088858	10.937434	-0.129794	4.817111
670.927199	8000.157975	10.942439	-0.129824	4.817131
671.617246	8000.414076	10.947443	-0.129953	4.817203
671.194300	8000.216057	10.952448	-0.129874	4.817147
671.041436	8000.398821	10.957453	-0.129846	4.817201
671.685946	8000.491308	10.962458	-0.129966	4.817226
671.690684	8000.496671	10.967463	-0.129967	4.817227
671.770290	8000.533872	10.972467	-0.129981	4.817238
671.560033	8000.422713	10.977472	-0.129942	4.817206
672.064369	8000.459081	10.982477	-0.130036	4.817214
671.648841	8000.476982	10.987482	-0.129959	4.817221
671.747278	8000.508127	10.992487	-0.129977	4.817230
671.237268	8000.289716	10.997491	-0.129882	4.817168
671.157121	8000.101234	11.002496	-0.129867	4.817113
671.087260	8000.296918	11.007501	-0.129854	4.817171
671.114361	8000.155582	11.012506	-0.129859	4.817129
671.189128	8000.108077	11.017511	-0.129873	4.817115
671.070506	8000.148557	11.022515	-0.129851	4.817127
670.958228	8000.202888	11.027520	-0.129830	4.817144
671.390201	8000.045599	11.032525	-0.129910	4.817095
671.629590	8000.404749	11.037530	-0.129955	4.817200
671.059858	8000.288032	11.042535	-0.129849	4.817168
671.113776	8000.224336	11.047539	-0.129859	4.817149
671.436163	8000.343573	11.052544	-0.129919	4.817183
670.981922	8000.224413	11.057549	-0.129834	4.817150
670.962874	8000.064382	11.062554	-0.129831	4.817103
671.106132	8000.224218	11.067559	-0.129858	4.817149
671.454771	8000.313183	11.072563	-0.129923	4.817174
671.224587	8000.341359	11.077568	-0.129880	4.817183
671.477049	8000.333628	11.082573	-0.129927	4.817180
672.051129	8000.368957	11.087578	-0.130034	4.817188
671.508764	8000.307672	11.092583	-0.129933	4.817172
671.295067	8000.191174	11.097587	-0.129893	4.817139
671.370647	7999.956438	11.102592	-0.129907	4.817069
671.551749	8000.336900	11.107597	-0.129941	4.817181
671.717317	8000.245310	11.112602	-0.129971	4.817153
671.567368	8000.523332	11.117607	-0.129944	4.817236
671.683520	8000.388660	11.122611	-0.129965	4.817195
671.907035	8000.387887	11.127616	-0.130007	4.817194
671.924085	8000.498173	11.132621	-0.130010	4.817226
671.706855	8000.253612	11.137626	-0.129969	4.817155
671.695977	8000.319033	11.142631	-0.129967	4.817175
671.974969	8000.501077	11.147635	-0.130020	4.817227
672.332391	8000.475930	11.152640	-0.130086	4.817218
672.093167	8000.362205	11.157645	-0.130041	4.817186
671.982320	8000.366838	11.162650	-0.130021	4.817187
671.832216	8000.389905	11.167655	-0.129993	4.817195
671.726436	8000.279305	11.172659	-0.129973	4.817163
671.666734	8000.327045	11.177664	-0.129962	4.817177
672.248680	8000.435493	11.182669	-0.130071	4.817207
672.352959	8000.474134	11.187674	-0.130090	4.817217
672.448088	8000.582457	11.192679	-0.130108	4.817249
672.467833	8000.416669	11.197683	-0.130111	4.817200
672.210235	8000.432782	11.202688	-0.130063	4.817206
671.783762	8000.479078	11.207693	-0.129984	4.817221
671.832484	8000.358174	11.212698	-0.129993	4.817186
672.111164	8000.404802	11.217703	-0.130045	4.817198
671.984228	8000.410243	11.222707	-0.130021	4.817200
671.986259	8000.380654	11.227712	-0.130022	4.817192
672.248404	8000.495791	11.232717	-0.130071	4.817224
672.283893	8000.308033	11.237722	-0.130077	4.817169
671.454010	8000.161901	11.242727	-0.129922	4.817129
671.515666	8000.072935	11.247731	-0.129934	4.817103
671.815981	8000.315604	11.252736	-0.129990	4.817173
671.706452	8000.332952	11.257741	-0.129970	4.817179
671.803147	8000.203269	11.262746	-0.129987	4.817140
671.703202	8000.326554	11.267751	-0.129969	4.817177
672.143001	8000.283638	11.272755	-0.130051	4.817162
672.038225	8000.290480	11.277760	-0.130031	4.817165
671.902911	8000.414277	11.282765	-0.130006	4.817202
672.181083	8000.381555	11.287770	-0.130058	4.817191
672.074293	8000.499446	11.292775	-0.130038	4.817226
671.694213	8000.299969	11.297779	-0.129967	4.817169
671.763939	8000.150828	11.302784	-0.129980	4.817125
671.863665	8000.203149	11.307789	-0.129999	4.817140
671.861367	8000.422098	11.312794	-0.129998	4.817204
671.755501	8000.231097	11.317799	-0.129979	4.817148
672.125163	8000.361648	11.322803	-0.130048	4.817185
672.353273	8000.455101	11.327808	-0.130090	4.817212
672.536364	8000.581713	11.332813	-0.130124	4.817248
672.535660	8000.390218	11.337818	-0.130124	4.817192
672.373869	8000.414162	11.342823	-0.130094	4.817200
672.084563	8000.282736	11.347827	-0.130040	4.817162
672.244120	8000.471397	11.352832	-0.130070	4.817217
672.623158	8000.438121	11.357837	-0.130140	4.817206
672.565019	8000.458380	11.362842	-0.130129	4.817212
672.423620	8000.479466	11.367847	-0.130103	4.817219
672.702381	8000.488013	11.372851	-0.130155	4.817220
672.653579	8000.475620	11.377856	-0.130146	4.817217
672.797262	8000.394269	11.382861	-0.130173	4.817192
672.854649	8000.446996	11.387866	-0.130183	4.817207
672.760807	8000.338693	11.392871	-0.130166	4.817176
672.768706	8000.503852	11.397875	-0.130167	4.817224
673.110311	8000.446723	11.402880	-0.130231	4.817206
673.165463	8000.554429	11.407885	-0.130241	4.817237
673.278507	8000.499051	11.412890	-0.130262	4.817221
673.112521	8000.448873	11.417895	-0.130231	4.817207
672.745620	8000.496090	11.422899	-0.130163	4.817222
672.920340	8000.364438	11.427904	-0.130196	4.817182
672.130911	8000.471764	11.432909	-0.130049	4.817218
672.601527	8000.262176	11.437914	-0.130136	4.817154
672.617618	8000.556526	11.442919	-0.130139	4.817241
672.442920	8000.405713	11.447923	-0.130107	4.817197
672.487755	8000.332353	11.452928	-0.130115	4.817175
672.397117	8000.431452	11.457933	-0.130098	4.817205
672.469651	8000.318321	11.462938	-0.130112	4.817171
672.345623	8000.421135	11.467943	-0.130089	4.817202
672.520931	8000.391053	11.472947	-0.130121	4.817192
673.064813	8000.506323	11.477952	-0.130223	4.817224
672.773907	8000.517688	11.482957	-0.130168	4.817228
672.628301	8000.228739	11.487962	-0.130141	4.817144
672.347507	8000.420107	11.492967	-0.130089	4.817202
672.463085	8000.464213	11.497971	-0.130111	4.817214
672.965822	8000.478343	11.502976	-0.130204	4.817216
672.846862	8000.495544	11.507981	-0.130182	4.817221
672.757724	8000.465600	11.512986	-0.130165	4.817213
672.903136	8000.489010	11.517991	-0.130193	4.817219
673.083684	8000.383897	11.522995	-0.130226	4.817187
672.818902	8000.236979	11.528000	-0.130177	4.817145
672.752917	8000.373487	11.533005	-0.130165	4.817186
673.424329	8000.504487	11.538010	-0.130290	4.817221
673.103501	8000.367278	11.543015	-0.130230	4.817182
672.680591	8000.413627	11.548019	-0.130151	4.817198
672.782333	8000.443766	11.553024	-0.130170	4.817207
672.615150	8000.211611	11.558029	-0.130139	4.817139
672.567379	8000.263768	11.563034	-0.130130	4.817154
672.571191	8000.324128	11.568039	-0.130131	4.817172
672.628234	8000.370501	11.573043	-0.130141	4.817186
672.656533	8000.246105	11.578048	-0.130146	4.817149
673.083992	8000.480176	11.583053	-0.130226	4.817216
672.832759	8000.384247	11.588058	-0.130179	4.817189
673.054523	8000.479720	11.593063	-0.130221	4.817216
672.696184	8000.221330	11.598067	-0.130154	4.817141
672.412586	8000.300516	11.603072	-0.130101	4.817166
672.336930	8000.221061	11.608077	-0.130087	4.817143
672.535124	8000.119395	11.613082	-0.130124	4.817112
672.661345	8000.341393	11.618087	-0.130147	4.817177
672.709423	8000.329443	11.623091	-0.130156	4.817173
672.593351	8000.314952	11.628096	-0.130135	4.817169
672.515088	8000.396258	11.633101	-0.130120	4.817194
673.046194	8000.448912	11.638106	-0.130219	4.817207
673.094561	8000.369259	11.643111	-0.130228	4.817183
672.839973	8000.303958	11.648115	-0.130181	4.817165
673.168469	8000.369345	11.653120	-0.130242	4.817183
673.250701	8000.464775	11.658125	-0.130257	4.817211
673.418889	8000.492770	11.663130	-0.130289	4.817218
673.405311	8000.491502	11.668135	-0.130286	4.817218
673.323435	8000.422526	11.673139	-0.130271	4.817198
673.788348	8000.539753	11.678144	-0.130357	4.817230
673.387326	8000.470065	11.683149	-0.130283	4.817212
673.647855	8000.313293	11.688154	-0.130331	4.817164
673.507969	8000.560802	11.693159	-0.130305	4.817238
673.734760	8000.402448	11.698163	-0.130347	4.817190
673.575028	8000.541740	11.703168	-0.130318	4.817232
673.881729	8000.426942	11.708173	-0.130375	4.817197
673.940404	8000.500849	11.713178	-0.130386	4.817218
673.750256	8000.512716	11.718183	-0.130350	4.817222
672.891785	8000.360833	11.723187	-0.130190	4.817182
673.119314	8000.216246	11.728192	-0.130233	4.817138
673.183862	8000.498655	11.733197	-0.130245	4.817221
672.719033	8000.350754	11.738202	-0.130158	4.817179
672.677561	8000.085635	11.743207	-0.130150	4.817101
672.789329	8000.320105	11.748211	-0.130171	4.817170
672.654188	7999.990063	11.753216	-0.130146	4.817073
672.883110	8000.345889	11.758221	-0.130189	4.817177
672.654668	7999.950929	11.763226	-0.130146	4.817062
672.840438	8000.360040	11.768231	-0.130181	4.817182
672.511913	8000.041816	11.773235	-0.130120	4.817089
673.202985	8000.109635	11.778240	-0.130248	4.817106
672.894070	8000.191604	11.783245	-0.130191	4.817132
672.925211	8000.198433	11.788250	-0.130197	4.817133
672.990111	8000.290419	11.793255	-0.130209	4.817160
672.806333	8000.128888	11.798259	-0.130174	4.817113
673.349329	8000.377441	11.803264	-0.130276	4.817184
673.184300	8000.398160	11.808269	-0.130245	4.817191
673.382900	8000.255241	11.813274	-0.130282	4.817148
673.160007	8000.415769	11.818279	-0.130240	4.817197
673.587274	8000.300722	11.823283	-0.130320	4.817161
673.504808	8000.370327	11.828288	-0.130305	4.817182
672.852073	8000.225867	11.833293	-0.130183	4.817142
672.783504	8000.037556	11.838298	-0.130170	4.817087
672.803433	8000.163756	11.843303	-0.130174	4.817124
673.202979	8000.333917	11.848307	-0.130248	4.817172
673.441314	8000.440227	11.853312	-0.130293	4.817202
673.395748	8000.476550	11.858317	-0.130284	4.817213
673.099822	8000.335494	11.863322	-0.130229	4.817173
673.641474	8000.488819	11.868327	-0.130330	4.817216
673.396417	8000.395099	11.873331	-0.130284	4.817189
673.149352	8000.351073	11.878336	-0.130238	4.817177
672.916051	8000.296681	11.883341	-0.130195	4.817162
673.301183	8000.333323	11.888346	-0.130267	4.817172
673.333069	8000.351802	11.893351	-0.130273	4.817177
673.321608	8000.314597	11.898355	-0.130271	4.817166
673.248105	8000.173813	11.903360	-0.130257	4.817125
673.131692	8000.256645	11.908365	-0.130235	4.817150
673.327515	8000.203606	11.913370	-0.130272	4.817133
673.379995	8000.311270	11.918375	-0.130281	4.817165
673.247685	8000.415015	11.923379	-0.130257	4.817196
673.323385	8000.400318	11.928384	-0.130271	4.817191
673.155103	8000.392423	11.933389	-0.130240	4.817190
673.674506	8000.510492	11.938394	-0.130336	4.817222
673.717125	8000.456139	11.943399	-0.130344	4.817206
674.154993	8000.515820	11.948403	-0.130426	4.817221
674.196128	8000.481544	11.953408	-0.130433	4.817211
673.876749	8000.544307	11.958413	-0.130374	4.817231
673.812338	8000.470310	11.963418	-0.130362	4.817210
673.781737	8000.497343	11.968423	-0.130356	4.817218
673.783541	8000.322810	11.973427	-0.130357	4.817166
673.405342	8000.364561	11.978432	-0.130286	4.817180
673.594623	8000.503967	11.983437	-0.130322	4.817221
673.438511	8000.192632	11.988442	-0.130292	4.817129
673.013796	8000.140569	11.993447	-0.130213	4.817116
673.369065	8000.191558	11.998451	-0.130279	4.817129
673.452452	8000.151589	12.003456	-0.130295	4.817117
673.032799	8000.345041	12.008461	-0.130217	4.817176
673.252324	8000.032122	12.013466	-0.130257	4.817083
672.999184	8000.151980	12.018471	-0.130210	4.817119
673.052821	8000.198301	12.023475	-0.130220	4.817133
672.987435	8000.148625	12.028480	-0.130208	4.817118
673.003482	8000.141468	12.033485	-0.130211	4.817116
673.555060	8000.408141	12.038490	-0.130314	4.817192
673.275123	8000.309651	12.043495	-0.130262	4.817165
673.724106	8000.382195	12.048499	-0.130346	4.817184
673.682679	8000.238732	12.053504	-0.130338	4.817142
673.796152	8000.510265	12.058509	-0.130359	4.817221
673.877693	8000.473442	12.063514	-0.130374	4.817210
674.007187	8000.448999	12.068519	-0.130398	4.817202
673.800992	8000.599209	12.073523	-0.130360	4.817248
673.750943	8000.269412	12.078528	-0.130351	4.817151
674.273442	8000.520834	12.083533	-0.130448	4.817222
673.774230	8000.345944	12.088538	-0.130355	4.817173
673.881913	8000.520058	12.093543	-0.130375	4.817224
674.099761	8000.372145	12.098547	-0.130416	4.817179
674.472884	8000.501707	12.103552	-0.130485	4.817216
674.086612	8000.469274	12.108557	-0.130413	4.817208
674.249985	8000.510950	12.113562	-0.130444	4.817220
674.003863	8000.377008	12.118567	-0.130398	4.817181
673.659905	8000.381203	12.123571	-0.130334	4.817184
673.802283	8000.238470	12.128576	-0.130360	4.817141
674.357503	8000.542239	12.133581	-0.130464	4.817228
674.499883	8000.443938	12.138586	-0.130490	4.817199
673.463818	8000.343256	12.143591	-0.130297	4.817174
674.172738	8000.431465	12.148595	-0.130429	4.817197
674.118670	8000.486700	12.153600	-0.130419	4.817213
673.912017	8000.498310	12.158605	-0.130381	4.817217
674.067932	8000.380118	12.163610	-0.130410	4.817182
673.963885	8000.373217	12.168615	-0.130390	4.817180
673.866439	8000.456344	12.173619	-0.130372	4.817205
674.178572	8000.496092	12.178624	-0.130430	4.817216
674.544654	8000.466851	12.183629	-0.130498	4.817205
674.820394	8000.470066	12.188634	-0.130550	4.817205
674.170758	8000.443074	12.193639	-0.130429	4.817200
674.193279	8000.517480	12.198643	-0.130433	4.817222
674.279367	8000.469089	12.203648	-0.130449	4.817207
674.140753	8000.517725	12.208653	-0.130423	4.817222
674.014200	8000.548561	12.213658	-0.130400	4.817232
673.929282	8000.495406	12.218663	-0.130384	4.817217
673.959270	8000.397481	12.223667	-0.130389	4.817187
673.972405	8000.398742	12.228672	-0.130392	4.817188
674.094171	8000.486323	12.233677	-0.130415	4.817213
673.952062	8000.141347	12.238682	-0.130388	4.817112
673.565506	8000.295111	12.243687	-0.130316	4.817159
673.295428	8000.239091	12.248691	-0.130266	4.817144
673.742001	8000.506260	12.253696	-0.130349	4.817221
673.616883	8000.381600	12.258701	-0.130326	4.817184
673.854999	8000.520706	12.263706	-0.130370	4.817224
674.170537	8000.440957	12.268711	-0.130429	4.817199
673.524744	8000.393927	12.273715	-0.130309	4.817188
674.102279	8000.370075	12.278720	-0.130416	4.817179
673.717756	8000.332382	12.283725	-0.130344	4.817169
674.179317	8000.389254	12.288730	-0.130430	4.817184
673.678585	8000.394194	12.293735	-0.130337	4.817188
673.513697	8000.194865	12.298739	-0.130306	4.817130
673.840556	8000.413630	12.303744	-0.130367	4.817193
674.027330	8000.550884	12.308749	-0.130402	4.817232
674.367837	8000.463058	12.313754	-0.130466	4.817205
674.402724	8000.567280	12.318759	-0.130472	4.817236
674.255590	8000.460262	12.323763	-0.130445	4.817205
673.955389	8000.402714	12.328768	-0.130389	4.817189
674.267591	8000.467854	12.333773	-0.130447	4.817207
674.378093	8000.465334	12.338778	-0.130468	4.817206
674.339459	8000.466852	12.343783	-0.130460	4.817206
673.851909	8000.478343	12.348787	-0.130370	4.817212
673.709667	8000.290999	12.353792	-0.130343	4.817157
674.297586	8000.429175	12.358797	-0.130453	4.817195
673.989437	8000.486821	12.363802	-0.130395	4.817214
674.251238	8000.505688	12.368807	-0.130444	4.817218
674.225904	8000.479905	12.373811	-0.130439	4.817211
673.953344	8000.294773	12.378816	-0.130388	4.817157
674.189853	8000.503680	12.383821	-0.130433	4.817218
674.424153	8000.475571	12.388826	-0.130476	4.817208
673.960569	8000.376348	12.393831	-0.130390	4.817181
674.194230	8000.381025	12.398835	-0.130433	4.817182
674.240842	8000.323560	12.403840	-0.130442	4.817164
674.240285	8000.449448	12.408845	-0.130442	4.817202
674.114574	8000.374502	12.413850	-0.130418	4.817180
674.321309	8000.392516	12.418855	-0.130457	4.817184
674.112415	8000.206255	12.423859	-0.130418	4.817130
674.049600	8000.245484	12.428864	-0.130406	4.817142
674.325006	8000.404211	12.433869	-0.130458	4.817188
674.259115	8000.184194	12.438874	-0.130445	4.817123
673.855339	8000.198044	12.443879	-0.130370	4.817129
674.409286	8000.371662	12.448883	-0.130473	4.817178
675.116870	8000.452452	12.453888	-0.130605	4.817198
674.500933	8000.573039	12.458893	-0.130491	4.817237
674.277487	8000.367506	12.463898	-0.130449	4.817177
674.648225	8000.460002	12.468903	-0.130518	4.817203
674.728044	8000.496152	12.473907	-0.130533	4.817213
674.099145	8000.173255	12.478912	-0.130415	4.817121
674.060256	8000.247767	12.483917	-0.130408	4.817143
674.232701	8000.122427	12.488922	-0.130440	4.817105
674.305123	8000.400731	12.493927	-0.130454	4.817187
674.163053	8000.284272	12.498931	-0.130427	4.817153
674.246314	8000.414632	12.503936	-0.130443	4.817191
673.914370	8000.130194	12.508941	-0.130381	4.817109
674.007849	8000.260710	12.513946	-0.130399	4.817147
674.023858	8000.159396	12.518951	-0.130401	4.817117
673.826632	7999.947931	12.523955	-0.130365	4.817055
673.993092	8000.095444	12.528960	-0.130396	4.817098
673.556015	8000.207166	12.533965	-0.130314	4.817133
673.628014	7999.977653	12.538970	-0.130328	4.817065
673.628076	8000.255889	12.543975	-0.130328	4.817147
673.334072	8000.059854	12.548979	-0.130273	4.817091
673.653467	8000.135678	12.553984	-0.130332	4.817112
673.988540	8000.357744	12.558989	-0.130395	4.817176
673.914995	8000.274085	12.563994	-0.130381	4.817151
673.728834	8000.134730	12.568999	-0.130347	4.817111
673.573735	8000.207442	12.574003	-0.130318	4.817133
673.683563	8000.008136	12.579008	-0.130338	4.817074
673.499512	8000.224278	12.584013	-0.130304	4.817138
673.248015	7999.979181	12.589018	-0.130257	4.817067
673.522726	8000.067007	12.594023	-0.130308	4.817092
673.553592	8000.122497	12.599027	-0.130314	4.817108
673.299130	7999.841387	12.604032	-0.130266	4.817026
673.730072	8000.143214	12.609037	-0.130347	4.817113
673.945176	8000.075662	12.614042	-0.130387	4.817093
674.053993	8000.150345	12.619047	-0.130407	4.817114
674.061946	8000.374752	12.624051	-0.130409	4.817180
673.975490	8000.236939	12.629056	-0.130393	4.817140
673.958226	8000.330828	12.634061	-0.130389	4.817168
674.173169	8000.084482	12.639066	-0.130429	4.817094
674.211840	8000.215208	12.644071	-0.130437	4.817133
674.070500	8000.219367	12.649075	-0.130410	4.817134
674.346835	8000.202488	12.654080	-0.130462	4.817128
674.162081	8000.364667	12.659085	-0.130427	4.817177
674.071776	8000.353747	12.664090	-0.130411	4.817174
674.225512	8000.124438	12.669095	-0.130439	4.817106
674.013247	8000.152890	12.674099	-0.130400	4.817115
674.195071	8000.132430	12.679104	-0.130433	4.817108
674.079772	8000.166615	12.684109	-0.130412	4.817119
674.097656	8000.173240	12.689114	-0.130415	4.817121
674.421808	8000.357054	12.694119	-0.130476	4.817173
674.292322	8000.402657	12.699123	-0.130452	4.817187
674.717493	8000.482244	12.704128	-0.130531	4.817209
674.347436	8000.413032	12.709133	-0.130462	4.817190
674.757325	8000.352730	12.714138	-0.130538	4.817171
674.260134	8000.274146	12.719143	-0.130446	4.817150
674.003613	8000.162264	12.724147	-0.130398	4.817118
674.025743	8000.108652	12.729152	-0.130402	4.817102
674.235830	8000.396493	12.734157	-0.130441	4.817186
674.496807	8000.306377	12.739162	-0.130490	4.817158
674.391239	8000.269830	12.744167	-0.130470	4.817148
674.727315	8000.474992	12.749171	-0.130533	4.817207
674.629109	8000.341224	12.754176	-0.130514	4.817168
674.599309	8000.483588	12.759181	-0.130509	4.817210
674.514434	8000.478041	12.764186	-0.130493	4.817209
674.619300	8000.483898	12.769191	-0.130513	4.817210
674.671848	8000.422292	12.774195	-0.130522	4.817192
674.534482	8000.518556	12.779200	-0.130497	4.817221
674.775929	8000.454587	12.784205	-0.130542	4.817201
674.722128	8000.492898	12.789210	-0.130532	4.817212
674.788665	8000.401886	12.794215	-0.130544	4.817185
674.262390	8000.384211	12.799219	-0.130446	4.817182
674.836310	8000.360305	12.804224	-0.130553	4.817172
674.833298	8000.484042	12.809229	-0.130553	4.817209
675.222856	8000.468919	12.814234	-0.130625	4.817203
674.802124	8000.312168	12.819239	-0.130547	4.817158
674.710405	8000.435587	12.824243	-0.130530	4.817195
674.650521	8000.296066	12.829248	-0.130518	4.817154
674.318186	8000.392482	12.834253	-0.130457	4.817184
674.855050	8000.387046	12.839258	-0.130557	4.817180
675.334102	8000.506616	12.844263	-0.130646	4.817213
674.941195	8000.483599	12.849267	-0.130573	4.817208
674.914819	8000.411248	12.854272	-0.130568	4.817187
674.138887	8000.255346	12.859277	-0.130423	4.817145
673.978050	8000.096281	12.864282	-0.130393	4.817098
674.282986	8000.321055	12.869287	-0.130450	4.817163
674.540900	8000.372659	12.874291	-0.130498	4.817177
674.566887	8000.190035	12.879296	-0.130503	4.817123
674.419776	8000.390884	12.884301	-0.130475	4.817183
674.307421	8000.287580	12.889306	-0.130454	4.817153
674.542532	8000.132529	12.894311	-0.130498	4.817107
674.572378	8000.254656	12.899315	-0.130504	4.817143
674.950752	8000.500677	12.904320	-0.130574	4.817213
675.101163	8000.488197	12.909325	-0.130602	4.817209
675.459606	8000.470476	12.914330	-0.130669	4.817202
675.133473	8000.471770	12.919335	-0.130608	4.817204
674.690182	8000.323133	12.924339	-0.130526	4.817162
675.382061	8000.459753	12.929344	-0.130655	4.817199
675.005799	8000.486720	12.934349	-0.130585	4.817209
674.436160	8000.328720	12.939354	-0.130479	4.817165
675.109329	8000.496788	12.944359	-0.130604	4.817212
675.154797	8000.452000	12.949363	-0.130612	4.817198
674.647756	8000.163783	12.954368	-0.130518	4.817115
675.034376	8000.449076	12.959373	-0.130590	4.817198
675.104134	8000.440635	12.964378	-0.130603	4.817195
675.413141	8000.445424	12.969383	-0.130661	4.817195
675.475478	8000.551132	12.974387	-0.130672	4.817226
675.399231	8000.385962	12.979392	-0.130658	4.817177
675.315291	8000.562404	12.984397	-0.130642	4.817230
674.911456	8000.503245	12.989402	-0.130567	4.817214
675.099697	8000.370741	12.994407	-0.130602	4.817174
674.726181	8000.257041	12.999411	-0.130532	4.817143
674.670123	8000.371491	13.004416	-0.130522	4.817177
674.701937	8000.470376	13.009421	-0.130528	4.817206
674.683106	8000.308215	13.014426	-0.130525	4.817158
674.732936	8000.514234	13.019431	-0.130534	4.817218
674.992561	8000.496040	13.024435	-0.130582	4.817212
674.588604	8000.277129	13.029440	-0.130507	4.817149
674.823312	8000.371750	13.034445	-0.130551	4.817176
674.848201	8000.518137	13.039450	-0.130555	4.817219
675.234018	8000.344259	13.044455	-0.130627	4.817166
675.307629	8000.507271	13.049459	-0.130641	4.817214
675.409646	8000.488751	13.054464	-0.130660	4.817208
675.190442	8000.508629	13.059469	-0.130619	4.817215
675.613891	8000.481337	13.064474	-0.130698	4.817205
675.736221	8000.557294	13.069479	-0.130721	4.817226
675.481636	8000.476114	13.074483	-0.130673	4.817204
675.166313	8000.233181	13.079488	-0.130614	4.817133
675.136907	8000.382959	13.084493	-0.130609	4.817178
675.202710	8000.411486	13.089498	-0.130621	4.817186
675.195862	8000.448409	13.094503	-0.130620	4.817197
675.292869	8000.454145	13.099507	-0.130638	4.817198
675.303611	8000.390832	13.104512	-0.130640	4.817179
674.964021	8000.509354	13.109517	-0.130577	4.817216
675.200726	8000.347977	13.114522	-0.130621	4.817167
675.153829	8000.359946	13.119527	-0.130612	4.817171
674.986741	8000.445170	13.124531	-0.130581	4.817197
674.955289	8000.355813	13.129536	-0.130575	4.817171
675.311533	8000.457609	13.134541	-0.130642	4.817199
675.070979	8000.394635	13.139546	-0.130597	4.817182
674.927912	8000.443201	13.144551	-0.130570	4.817197
675.301270	8000.460625	13.149555	-0.130640	4.817200
675.518661	8000.413211	13.154560	-0.130680	4.817185
675.004351	8000.405241	13.159565	-0.130584	4.817185
675.164510	8000.377041	13.164570	-0.130614	4.817176
675.511556	8000.426855	13.169575	-0.130679	4.817189
675.570842	8000.491254	13.174579	-0.130690	4.817208
675.493668	8000.471014	13.179584	-0.130676	4.817202
675.078746	8000.270974	13.184589	-0.130598	4.817145
675.315174	8000.593091	13.189594	-0.130642	4.817239
675.236681	8000.410958	13.194599	-0.130628	4.817186
675.440916	8000.544257	13.199603	-0.130666	4.817224
675.692602	8000.488911	13.204608	-0.130713	4.817207
675.664553	8000.505404	13.209613	-0.130707	4.817212
675.760742	8000.355601	13.214618	-0.130725	4.817167
675.782384	8000.576001	13.219623	-0.130729	4.817232
675.242815	8000.509447	13.224627	-0.130629	4.817215
674.483461	8000.048048	13.229632	-0.130487	4.817082
674.583734	8000.228395	13.234637	-0.130506	4.817135
674.762491	8000.260787	13.239642	-0.130539	4.817143
674.617205	8000.105133	13.244647	-0.130512	4.817098
674.768441	8000.365618	13.249651	-0.130541	4.817174
675.164303	8000.405607	13.254656	-0.130614	4.817184
675.270339	8000.466497	13.259661	-0.130634	4.817202
674.958629	8000.254304	13.264666	-0.130576	4.817141
675.199510	8000.501372	13.269671	-0.130621	4.817212
675.361753	8000.371638	13.274675	-0.130651	4.817173
675.126932	8000.497073	13.279680	-0.130607	4.817212
674.894921	8000.388738	13.284685	-0.130564	4.817181
675.450028	8000.365601	13.289690	-0.130667	4.817171
675.134286	8000.436883	13.294695	-0.130609	4.817194
675.288330	8000.419168	13.299699	-0.130637	4.817188
675.321759	8000.475760	13.304704	-0.130644	4.817204
675.314013	8000.395233	13.309709	-0.130642	4.817181
675.118217	8000.313909	13.314714	-0.130606	4.817157
675.541247	8000.391349	13.319719	-0.130684	4.817178
675.123243	8000.233581	13.324723	-0.130607	4.817134
675.187018	8000.272656	13.329728	-0.130618	4.817145
674.825328	8000.268111	13.334733	-0.130551	4.817145
675.431285	8000.477459	13.339738	-0.130664	4.817204
675.345216	8000.483531	13.344743	-0.130648	4.817207
675.256341	8000.468400	13.349747	-0.130631	4.817202
675.708674	8000.466947	13.354752	-0.130716	4.817200
675.463485	8000.440929	13.359757	-0.130670	4.817193
675.957179	8000.508888	13.364762	-0.130762	4.817211
675.733485	8000.478970	13.369767	-0.130720	4.817203
675.164422	8000.396091	13.374771	-0.130614	4.817182
675.083167	8000.239310	13.379776	-0.130599	4.817136
675.344549	8000.452840	13.384781	-0.130648	4.817197
675.504250	8000.390778	13.389786	-0.130678	4.817178
675.516940	8000.384627	13.394791	-0.130680	4.817177
675.626849	8000.446636	13.399795	-0.130700	4.817194
675.788096	8000.421628	13.404800	-0.130731	4.817186
675.859627	8000.595192	13.409805	-0.130744	4.817237
675.773940	8000.477483	13.414810	-0.130728	4.817203
675.461967	8000.445140	13.419815	-0.130670	4.817195
675.661850	8000.489500	13.424819	-0.130707	4.817207
675.497337	8000.392789	13.429824	-0.130676	4.817179
675.821079	8000.528999	13.434829	-0.130737	4.817218
675.558842	8000.463570	13.439834	-0.130688	4.817200
675.508586	8000.522039	13.444839	-0.130679	4.817217
675.602775	8000.509745	13.449843	-0.130696	4.817213
675.922614	8000.458629	13.454848	-0.130756	4.817197
676.264158	8000.478737	13.459853	-0.130819	4.817201
676.199011	8000.510525	13.464858	-0.130807	4.817211
675.736084	8000.402838	13.469863	-0.130721	4.817181
676.155911	8000.482349	13.474867	-0.130799	4.817202
676.158899	8000.448539	13.479872	-0.130800	4.817192
676.119079	8000.534679	13.484877	-0.130792	4.817218
675.942687	8000.433550	13.489882	-0.130759	4.817189
675.776458	8000.572745	13.494887	-0.130728	4.817231
675.506824	8000.389764	13.499891	-0.130678	4.817178
676.139626	8000.519128	13.504896	-0.130796	4.817213
675.645684	8000.440584	13.509901	-0.130704	4.817192
675.464729	8000.400750	13.514906	-0.130670	4.817182
675.718447	8000.453351	13.519911	-0.130718	4.817196
675.467162	8000.447340	13.524915	-0.130671	4.817195
675.434830	8000.339982	13.529920	-0.130665	4.817164
675.304457	8000.384513	13.534925	-0.130640	4.817177
676.091881	8000.439038	13.539930	-0.130787	4.817190
675.410947	8000.491963	13.544935	-0.130660	4.817209
675.578011	8000.377115	13.549939	-0.130691	4.817174
675.874256	8000.480101	13.554944	-0.130747	4.817203
675.782714	8000.433188	13.559949	-0.130730	4.817190
675.951971	8000.500351	13.564954	-0.130761	4.817209
675.916336	8000.423622	13.569959	-0.130754	4.817186
675.477264	8000.416816	13.574963	-0.130673	4.817186
675.042159	8000.309566	13.579968	-0.130592	4.817157
675.611255	8000.391386	13.584973	-0.130698	4.817178
675.382464	8000.231259	13.589978	-0.130655	4.817132
675.079819	8000.258309	13.594983	-0.130599	4.817141
675.014300	8000.261526	13.599987	-0.130586	4.817143
675.512707	8000.360235	13.604992	-0.130679	4.817169
675.452365	8000.501071	13.609997	-0.130668	4.817211
675.023426	8000.263784	13.615002	-0.130588	4.817143
675.459260	8000.365756	13.620007	-0.130669	4.817171
675.407245	8000.492967	13.625011	-0.130660	4.817209
675.372048	8000.231099	13.630016	-0.130653	4.817132
674.981065	8000.302274	13.635021	-0.130580	4.817155
675.416397	8000.383078	13.640026	-0.130661	4.817177
675.148568	8000.313333	13.645031	-0.130611	4.817157
675.492693	8000.389551	13.650035	-0.130676	4.817178
675.521340	8000.195326	13.655040	-0.130681	4.817121
675.586880	8000.374083	13.660045	-0.130693	4.817173
675.014800	8000.194885	13.665050	-0.130586	4.817123
675.374427	8000.213152	13.670055	-0.130653	4.817127
675.463934	8000.505485	13.675059	-0.130670	4.817212
675.628278	8000.404349	13.680064	-0.130701	4.817182
675.351174	8000.409576	13.685069	-0.130649	4.817185
676.171946	8000.442401	13.690074	-0.130802	4.817191
675.775562	8000.484924	13.695079	-0.130728	4.817205
675.463258	8000.412372	13.700083	-0.130670	4.817185
675.689935	8000.496293	13.705088	-0.130712	4.817209
675.869231	8000.434535	13.710093	-0.130746	4.817190
675.798099	8000.439780	13.715098	-0.130733	4.817192
675.646630	8000.403577	13.720103	-0.130704	4.817182
675.305435	8000.351738	13.725107	-0.130641	4.817168
675.629745	8000.340894	13.730112	-0.130701	4.817163
675.384958	8000.379420	13.735117	-0.130656	4.817176
675.426358	8000.419207	13.740122	-0.130663	4.817187
675.433316	8000.373822	13.745127	-0.130665	4.817174
675.107461	8000.295772	13.750131	-0.130604	4.817152
675.134006	8000.327923	13.755136	-0.130609	4.817162
675.423313	8000.332406	13.760141	-0.130663	4.817162
675.379402	8000.195247	13.765146	-0.130654	4.817121
674.941648	8000.201161	13.770151	-0.130573	4.817125
675.248847	8000.407994	13.775155	-0.130630	4.817185
675.403274	8000.131081	13.780160	-0.130659	4.817102
675.135642	8000.514154	13.785165	-0.130609	4.817217
675.110831	8000.159348	13.790170	-0.130604	4.817112
675.416535	8000.299505	13.795175	-0.130661	4.817152
675.227674	8000.317738	13.800179	-0.130626	4.817158
675.621004	8000.302674	13.805184	-0.130699	4.817152
675.586194	8000.364556	13.810189	-0.130693	4.817170
675.564637	8000.352584	13.815194	-0.130689	4.817167
675.409019	8000.154447	13.820199	-0.130660	4.817109
675.991800	8000.488282	13.825203	-0.130769	4.817205
675.721274	8000.335968	13.830208	-0.130718	4.817161
675.072253	8000.342839	13.835213	-0.130597	4.817166
675.281934	8000.282609	13.840218	-0.130636	4.817148
675.488316	8000.371504	13.845223	-0.130675	4.817173
675.009460	8000.129215	13.850227	-0.130586	4.817103
675.041355	8000.100086	13.855232	-0.130591	4.817095
675.264514	8000.380732	13.860237	-0.130633	4.817177
675.213299	8000.084764	13.865242	-0.130623	4.817089
675.472406	8000.319417	13.870247	-0.130672	4.817157
675.530702	8000.441989	13.875251	-0.130683	4.817193
675.608357	8000.272857	13.880256	-0.130697	4.817143
675.049560	8000.206011	13.885261	-0.130593	4.817126
675.106188	8000.176207	13.890266	-0.130604	4.817117
675.388481	8000.268392	13.895271	-0.130656	4.817143
674.811766	8000.036229	13.900275	-0.130549	4.817077
674.956076	8000.000378	13.905280	-0.130576	4.817066
674.878414	8000.029856	13.910285	-0.130561	4.817075
675.347349	8000.240248	13.915290	-0.130649	4.817135
675.430900	8000.198166	13.920295	-0.130664	4.817122
675.475352	8000.294073	13.925299	-0.130672	4.817150
675.366965	7999.940090	13.930304	-0.130652	4.817046
675.147739	8000.160983	13.935309	-0.130611	4.817112
675.298234	8000.228909	13.940314	-0.130639	4.817132
675.166673	8000.133769	13.945319	-0.130615	4.817104
675.207733	8000.300507	13.950323	-0.130623	4.817153
675.317308	8000.233437	13.955328	-0.130643	4.817133
675.057776	8000.263271	13.960333	-0.130595	4.817143
675.338604	8000.100463	13.965338	-0.130647	4.817093
675.116417	8000.029312	13.970343	-0.130605	4.817074
675.222170	8000.216094	13.975347	-0.130625	4.817128
674.953080	8000.057463	13.980352	-0.130575	4.817083
675.639475	8000.338938	13.985357	-0.130703	4.817162
675.346661	8000.266690	13.990362	-0.130648	4.817143
675.380011	8000.196322	13.995367	-0.130655	4.817122
675.154330	8000.075392	14.000371	-0.130613	4.817087
675.006636	7999.993759	14.005376	-0.130585	4.817064
674.993658	8000.030586	14.010381	-0.130583	4.817074
675.718316	8000.218493	14.015386	-0.130718	4.817127
675.498902	8000.223557	14.020391	-0.130677	4.817129
675.455772	8000.282136	14.025395	-0.130669	4.817147
675.811273	8000.132121	14.030400	-0.130735	4.817101
675.848336	8000.497703	14.035405	-0.130742	4.817208
675.634505	8000.284906	14.040410	-0.130702	4.817147
675.974266	8000.380101	14.045415	-0.130765	4.817173
676.082907	8000.445266	14.050419	-0.130786	4.817192
676.050332	8000.437355	14.055424	-0.130780	4.817190
675.817573	8000.348049	14.060429	-0.130736	4.817164
675.617800	8000.385157	14.065434	-0.130699	4.817176
675.911434	8000.410868	14.070439	-0.130754	4.817182
675.439906	8000.365472	14.075443	-0.130666	4.817171
675.769192	8000.339894	14.080448	-0.130727	4.817162
675.574655	8000.392953	14.085453	-0.130691	4.817179
675.342249	8000.052915	14.090458	-0.130648	4.817079
676.160428	8000.377699	14.095463	-0.130800	4.817172
675.967854	8000.498500	14.100467	-0.130764	4.817208
675.620803	8000.248724	14.105472	-0.130700	4.817136
675.916529	8000.380267	14.110477	-0.130755	4.817173
676.301657	8000.493096	14.115482	-0.130826	4.817205
676.611067	8000.457690	14.120487	-0.130884	4.817193
676.327571	8000.462816	14.125491	-0.130831	4.817196
676.663191	8000.469079	14.130496	-0.130894	4.817196
676.317399	8000.592795	14.135501	-0.130829	4.817234
676.404441	8000.421688	14.140506	-0.130846	4.817183
676.485262	8000.426115	14.145511	-0.130861	4.817184
676.550229	8000.499068	14.150515	-0.130873	4.817206
676.463655	8000.499842	14.155520	-0.130857	4.817206
676.603804	8000.409968	14.160525	-0.130883	4.817179
676.370171	8000.555526	14.165530	-0.130839	4.817223
676.465056	8000.478704	14.170535	-0.130857	4.817200
676.042123	8000.426652	14.175539	-0.130778	4.817187
676.120171	8000.235306	14.180544	-0.130793	4.817130
676.321589	8000.470132	14.185549	-0.130830	4.817198
676.403035	8000.475627	14.190554	-0.130845	4.817199
676.082180	8000.435738	14.195559	-0.130786	4.817189
675.843293	8000.300843	14.200563	-0.130741	4.817150
676.115291	8000.310349	14.205568	-0.130792	4.817152
676.149531	8000.419854	14.210573	-0.130798	4.817184
676.478330	8000.488434	14.215578	-0.130859	4.817203
676.498258	8000.495091	14.220583	-0.130863	4.817205
676.410278	8000.418608	14.225587	-0.130847	4.817182
676.329261	8000.313667	14.230592	-0.130832	4.817152
676.396115	8000.491391	14.235597	-0.130844	4.817204
676.554061	8000.451520	14.240602	-0.130874	4.817192
676.606369	8000.473492	14.245607	-0.130883	4.817198
676.240631	8000.502735	14.250611	-0.130815	4.817208
676.438547	8000.480412	14.255616	-0.130852	4.817201
675.925688	8000.417444	14.260621	-0.130756	4.817184
676.514851	8000.394838	14.265626	-0.130866	4.817175
676.372810	8000.464581	14.270631	-0.130840	4.817196
676.377944	8000.461487	14.275635	-0.130841	4.817195
676.496850	8000.437938	14.280640	-0.130863	4.817188
676.501788	8000.490916	14.285645	-0.130864	4.817203
676.119143	8000.470171	14.290650	-0.130793	4.817199
676.238792	8000.384211	14.295655	-0.130815	4.817173
676.799867	8000.422535	14.300659	-0.130919	4.817182
676.821992	8000.445097	14.305664	-0.130923	4.817188
676.249490	8000.581168	14.310669	-0.130817	4.817231
676.132652	8000.411133	14.315674	-0.130795	4.817182
675.666826	8000.218764	14.320679	-0.130708	4.817127
675.765789	8000.294357	14.325683	-0.130727	4.817149
676.158526	8000.418940	14.330688	-0.130800	4.817184
675.698374	8000.132499	14.335693	-0.130714	4.817101
676.023929	8000.319518	14.340698	-0.130775	4.817155
675.618922	8000.250820	14.345703	-0.130699	4.817137
676.080498	8000.408209	14.350707	-0.130785	4.817181
676.134093	8000.316994	14.355712	-0.130795	4.817154
676.086742	8000.369160	14.360717	-0.130786	4.817169
676.125862	8000.296765	14.365722	-0.130794	4.817148
676.364269	8000.322679	14.370727	-0.130838	4.817154
676.194208	8000.194141	14.375731	-0.130806	4.817117
676.412052	8000.346696	14.380736	-0.130847	4.817161
676.539583	8000.388878	14.385741	-0.130871	4.817173
676.346125	8000.268440	14.390746	-0.130835	4.817138
676.111287	8000.234118	14.395751	-0.130791	4.817129
675.940480	7999.465504	14.400755	-0.130759	4.816903

675.884341	7996.339784	14.405760	-0.130746	4.815981
675.247334	7990.728198	14.410765	-0.130624	4.814327
675.629101	7984.031712	14.415770	-0.130691	4.812348
675.988517	7976.730056	14.420775	-0.130753	4.810189
676.016360	7969.056022	14.425779	-0.130753	4.807921
675.748228	7961.303196	14.430784	-0.130698	4.805629
675.980120	7953.414720	14.435789	-0.130736	4.803294
675.982594	7945.488791	14.440794	-0.130731	4.800948
675.938623	7937.523938	14.445799	-0.130718	4.798589
676.048611	7929.509320	14.450803	-0.130733	4.796214
676.341680	7921.492702	14.455808	-0.130783	4.793836
675.445538	7913.630304	14.460813	-0.130611	4.791508
675.718680	7905.483533	14.465818	-0.130656	4.789089
675.686198	7897.559681	14.470823	-0.130645	4.786737
675.637107	7889.440937	14.475827	-0.130631	4.784326
675.740176	7881.531979	14.480832	-0.130645	4.781975
675.761044	7873.470500	14.485837	-0.130643	4.779578
675.329421	7865.541832	14.490842	-0.130558	4.777221
675.024803	7857.569492	14.495847	-0.130496	4.774849
675.087025	7849.489235	14.500851	-0.130502	4.772442
674.999580	7841.520248	14.505856	-0.130481	4.770068
675.333168	7833.468991	14.510861	-0.130537	4.767667
675.417900	7825.409453	14.515866	-0.130548	4.765263
675.127438	7817.524499	14.520871	-0.130489	4.762911
675.380573	7809.435132	14.525875	-0.130531	4.760496
675.004326	7801.493548	14.530880	-0.130455	4.758125
675.378692	7793.438599	14.535885	-0.130520	4.755716
675.137715	7785.472095	14.540890	-0.130470	4.753335
675.496733	7777.445823	14.545895	-0.130531	4.750933
674.949568	7769.414525	14.550899	-0.130424	4.748531
675.401850	7761.433675	14.555904	-0.130503	4.746140
674.589816	7753.433218	14.560909	-0.130347	4.743745
674.787024	7745.469415	14.565914	-0.130378	4.741358
674.569756	7737.480804	14.570919	-0.130333	4.738963
674.012139	7729.471449	14.575923	-0.130224	4.736561
674.454016	7721.379438	14.580928	-0.130301	4.734130
674.673230	7713.430849	14.585933	-0.130336	4.731742
674.291028	7705.349285	14.590938	-0.130260	4.729315
674.503797	7697.400396	14.595943	-0.130294	4.726924
674.552786	7689.328610	14.600947	-0.130298	4.724496
674.787896	7681.418996	14.605952	-0.130337	4.722115
674.660572	7673.346787	14.610957	-0.130308	4.719684
674.463441	7665.442999	14.615962	-0.130266	4.717303
674.437819	7657.400588	14.620967	-0.130256	4.714879
674.164030	7649.392685	14.625971	-0.130200	4.712465
673.831527	7641.438253	14.630976	-0.130133	4.710065
674.244115	7633.376085	14.635981	-0.130204	4.707630
674.034841	7625.379070	14.640986	-0.130160	4.705215
674.534686	7617.372045	14.645991	-0.130248	4.702794
674.522205	7609.347310	14.650995	-0.130240	4.700368
674.644156	7601.372906	14.656000	-0.130258	4.697955
674.597922	7593.351091	14.661005	-0.130244	4.695527
674.306314	7585.374381	14.666010	-0.130185	4.693112
674.436339	7577.413367	14.671015	-0.130204	4.690700
674.406851	7569.352648	14.676019	-0.130193	4.688256
674.266822	7561.392349	14.681024	-0.130162	4.685842
674.382422	7553.391115	14.686029	-0.130178	4.683413
674.162758	7545.458298	14.691034	-0.130132	4.681005
673.997611	7537.443584	14.696039	-0.130096	4.678571
673.362802	7529.452779	14.701043	-0.129973	4.676143
673.378264	7521.423723	14.706048	-0.129970	4.673701
673.583397	7513.351345	14.711053	-0.130003	4.671244
673.518879	7505.343726	14.716058	-0.129986	4.668807
673.974862	7497.353293	14.721063	-0.130066	4.666373
673.606132	7489.344871	14.726067	-0.129992	4.663932
673.551918	7481.417446	14.731072	-0.129976	4.661515
673.684588	7473.314594	14.736077	-0.129996	4.659043
673.210356	7465.419006	14.741082	-0.129902	4.656634
673.218713	7457.354033	14.746087	-0.129899	4.654171
672.935110	7449.425518	14.751091	-0.129841	4.651748
673.266039	7441.355401	14.756096	-0.129897	4.649281
672.708102	7433.422626	14.761101	-0.129788	4.646855
673.127940	7425.265204	14.766106	-0.129861	4.644358
673.072582	7417.410054	14.771111	-0.129846	4.641953
673.142083	7409.330932	14.776115	-0.129853	4.639478
672.494218	7401.477418	14.781120	-0.129727	4.637071
672.903429	7393.302327	14.786125	-0.129798	4.634564
673.165983	7385.351140	14.791130	-0.129842	4.632124
673.396296	7377.300340	14.796135	-0.129880	4.629652
672.785618	7369.346097	14.801139	-0.129761	4.627209
673.116530	7361.310953	14.806144	-0.129817	4.624739
672.835878	7353.437453	14.811149	-0.129760	4.622318
673.006157	7345.293078	14.816154	-0.129786	4.619813
672.985427	7337.409707	14.821159	-0.129777	4.617386
672.793398	7329.336066	14.826163	-0.129736	4.614899
672.387015	7321.396721	14.831168	-0.129655	4.612452
672.403226	7313.303327	14.836173	-0.129653	4.609957
672.748576	7305.289733	14.841178	-0.129712	4.607485
672.924882	7297.294742	14.846183	-0.129740	4.605017
672.912461	7289.283091	14.851187	-0.129732	4.602543
672.924270	7281.369655	14.856192	-0.129729	4.600098
672.553309	7273.414825	14.861197	-0.129655	4.597639
672.478106	7265.331518	14.866202	-0.129636	4.595138
672.453051	7257.351351	14.871207	-0.129626	4.592668
672.812023	7249.248440	14.876211	-0.129687	4.590159
672.853768	7241.314971	14.881216	-0.129690	4.587702
672.583634	7233.265909	14.886221	-0.129635	4.585206
672.617568	7225.288751	14.891226	-0.129636	4.582732
672.415353	7217.325786	14.896231	-0.129593	4.580261
672.249725	7209.313794	14.901235	-0.129557	4.577773
672.052925	7201.330465	14.906240	-0.129515	4.575292
671.827317	7193.314518	14.911245	-0.129468	4.572800
671.951815	7185.226257	14.916250	-0.129486	4.570285
672.337160	7177.282651	14.921255	-0.129552	4.567813
671.959815	7169.265600	14.926259	-0.129477	4.565317
671.884658	7161.303706	14.931264	-0.129457	4.562836
671.585626	7153.352328	14.936269	-0.129397	4.560357
672.175900	7145.257572	14.941274	-0.129501	4.557834
672.133533	7137.298583	14.946279	-0.129488	4.555350
671.639592	7129.285547	14.951283	-0.129391	4.552848
671.745665	7121.251607	14.956288	-0.129406	4.550338
671.747926	7113.251657	14.961293	-0.129401	4.547838
671.705442	7105.191521	14.966298	-0.129388	4.545317
671.743638	7097.224137	14.971303	-0.129389	4.542824
671.619428	7089.250238	14.976307	-0.129361	4.540328
671.569016	7081.299207	14.981312	-0.129347	4.537837
671.009634	7073.285455	14.986317	-0.129237	4.535324
670.745505	7065.317030	14.991322	-0.129183	4.532825
671.131786	7057.225921	14.996327	-0.129250	4.530287
671.087896	7049.237927	15.001331	-0.129236	4.527779
671.312450	7041.170806	15.006336	-0.129273	4.525245
671.245684	7033.236579	15.011341	-0.129255	4.522751
671.082520	7025.224185	15.016346	-0.129219	4.520231
671.204810	7017.212938	15.021351	-0.129237	4.517711
671.161952	7009.214483	15.026355	-0.129224	4.515193
671.170763	7001.289419	15.031360	-0.129220	4.512696
670.249315	6993.306807	15.036365	-0.129044	4.510178
670.242824	6985.217683	15.041370	-0.129037	4.507627
670.810087	6977.155455	15.046375	-0.129137	4.505085
671.138344	6969.145331	15.051379	-0.129193	4.502557
670.622695	6961.196251	15.056384	-0.129092	4.500044
671.148510	6953.134785	15.061389	-0.129185	4.497498
671.198410	6945.131872	15.066394	-0.129189	4.494967
670.753559	6937.240178	15.071399	-0.129101	4.492469
670.797097	6929.153695	15.076403	-0.129104	4.489909
670.636658	6921.201107	15.081408	-0.129069	4.487389
670.042277	6913.201679	15.086413	-0.128953	4.484851
670.285430	6905.194738	15.091418	-0.128993	4.482313
670.711665	6897.155744	15.096423	-0.129067	4.479763
670.822221	6889.143483	15.101427	-0.129082	4.477220
670.922414	6881.142740	15.106432	-0.129096	4.474678
670.536770	6873.206305	15.111437	-0.129019	4.472154
670.171406	6865.164355	15.116442	-0.128946	4.469595
670.015027	6857.174612	15.121447	-0.128911	4.467052
670.021879	6849.135497	15.126451	-0.128907	4.464492
669.812503	6841.257549	15.131456	-0.128863	4.461982
669.714549	6833.132042	15.136461	-0.128840	4.459391
670.109202	6825.119342	15.141466	-0.128908	4.456837
670.616352	6817.046026	15.146471	-0.128997	4.454262
670.441429	6809.099755	15.151475	-0.128959	4.451724
670.172805	6801.113463	15.156480	-0.128904	4.449171
669.929321	6793.159833	15.161485	-0.128854	4.446628
670.142302	6785.075647	15.166490	-0.128888	4.444043
669.625203	6777.241506	15.171495	-0.128787	4.441533
669.317388	6769.149742	15.176499	-0.128724	4.438940
669.857146	6761.161460	15.181504	-0.128819	4.436383
669.443484	6753.176151	15.186509	-0.128737	4.433821
669.456163	6745.133767	15.191514	-0.128734	4.431240
669.987524	6737.074558	15.196519	-0.128828	4.428656
670.279063	6729.045901	15.201523	-0.128877	4.426079
669.906452	6721.128331	15.206528	-0.128802	4.423533
669.774217	6713.141790	15.211533	-0.128773	4.420964
669.297252	6705.158679	15.216538	-0.128679	4.418393
669.523033	6697.070141	15.221543	-0.128715	4.415790
669.727207	6689.032182	15.226547	-0.128748	4.413202
669.671536	6681.071930	15.231552	-0.128733	4.410636
669.045982	6673.146229	15.236557	-0.128611	4.408076
669.090058	6665.070871	15.241562	-0.128614	4.405471
668.959069	6657.117351	15.246567	-0.128584	4.402902
669.023475	6649.086888	15.251571	-0.128591	4.400308
669.332041	6641.028854	15.256576	-0.128643	4.397705
669.087373	6633.069250	15.261581	-0.128593	4.395129
669.142918	6625.100348	15.266586	-0.128598	4.392550
669.461935	6617.050374	15.271591	-0.128652	4.389945
669.020685	6609.102802	15.276595	-0.128565	4.387367
669.559180	6601.011005	15.281600	-0.128660	4.384747
669.292921	6593.127478	15.286605	-0.128605	4.382188
668.961824	6585.055672	15.291610	-0.128538	4.379566
669.167528	6577.104460	15.296615	-0.128571	4.376984
669.048941	6569.050804	15.301619	-0.128544	4.374366
669.259650	6561.106937	15.306624	-0.128578	4.371784
668.978228	6553.064195	15.311629	-0.128520	4.369166
668.927196	6545.110966	15.316634	-0.128505	4.366576
669.134997	6537.039440	15.321639	-0.128539	4.363948
668.942135	6529.113920	15.326643	-0.128498	4.361363
668.816347	6521.126740	15.331648	-0.128469	4.358757
668.342585	6513.201318	15.336653	-0.128376	4.356168
668.519670	6505.088497	15.341658	-0.128403	4.353519
668.717120	6497.055579	15.346663	-0.128435	4.350896
668.037396	6489.097633	15.351667	-0.128303	4.348289
668.360443	6481.064074	15.356672	-0.128358	4.345664
667.861986	6473.128358	15.361677	-0.128260	4.343062
668.428421	6465.078101	15.366682	-0.128360	4.340430
667.963216	6457.193328	15.371687	-0.128269	4.337842
668.065303	6449.130485	15.376691	-0.128282	4.335199
667.622826	6441.174146	15.381696	-0.128195	4.332585
667.720841	6433.122165	15.386701	-0.128208	4.329941
667.804122	6425.118155	15.391706	-0.128218	4.327312
667.937638	6417.133018	15.396711	-0.128238	4.324688
667.809021	6409.145481	15.401715	-0.128209	4.322060
668.024085	6401.079910	15.406720	-0.128243	4.319407
667.729572	6393.184759	15.411725	-0.128183	4.316804
667.545179	6385.129925	15.416730	-0.128144	4.314149
667.955225	6377.165259	15.421735	-0.128215	4.311525
667.692194	6369.062643	15.426739	-0.128161	4.308850
667.829818	6361.131239	15.431744	-0.128181	4.306232
667.716062	6353.074741	15.436749	-0.128155	4.303570
667.399033	6345.115180	15.441754	-0.128091	4.300936
667.761277	6337.080458	15.446759	-0.128153	4.298282
667.561620	6329.090154	15.451763	-0.128110	4.295635
666.907252	6321.148431	15.456768	-0.127983	4.293000
667.312343	6313.042581	15.461773	-0.128054	4.290317
667.406716	6305.072943	15.466778	-0.128066	4.287675
667.350838	6297.081982	15.471783	-0.128050	4.285023
667.453988	6289.059882	15.476787	-0.128064	4.282361
667.299003	6281.120931	15.481792	-0.128030	4.279722
667.160783	6273.137679	15.486797	-0.127999	4.277067
666.878127	6265.118268	15.491802	-0.127941	4.274397
666.447841	6257.152034	15.496807	-0.127856	4.271742
666.862048	6249.016236	15.501811	-0.127928	4.269036
666.647038	6241.101155	15.506816	-0.127883	4.266397
666.160160	6233.150808	15.511821	-0.127787	4.263741
666.831162	6225.030453	15.516826	-0.127907	4.261038
666.955152	6217.057366	15.521831	-0.127925	4.258377
666.763131	6209.070999	15.526835	-0.127884	4.255707
666.579516	6201.093227	15.531840	-0.127844	4.253038
666.495394	6193.087856	15.536845	-0.127823	4.250359
665.989455	6185.089406	15.541850	-0.127724	4.247677
666.484463	6177.057092	15.546855	-0.127811	4.244992
666.155883	6169.134607	15.551859	-0.127744	4.242333
666.471159	6161.060667	15.556864	-0.127798	4.239629
666.088258	6153.149027	15.561869	-0.127721	4.236970
665.859538	6145.093881	15.566874	-0.127674	4.234263
666.218817	6137.127698	15.571879	-0.127735	4.231590
665.576523	6129.089724	15.576883	-0.127611	4.228881
665.568075	6121.080692	15.581888	-0.127604	4.226186
665.703908	6113.091861	15.586893	-0.127624	4.223498
665.629532	6105.086707	15.591898	-0.127605	4.220801
665.951557	6097.075426	15.596903	-0.127659	4.218104
665.545935	6089.083369	15.601907	-0.127579	4.215404
665.993123	6081.045967	15.606912	-0.127657	4.212696
665.630225	6073.063006	15.611917	-0.127584	4.209996
665.872803	6065.010793	15.616922	-0.127624	4.207277
666.187571	6057.037080	15.621927	-0.127677	4.204584
665.758540	6049.101352	15.626931	-0.127592	4.201894
665.702343	6041.066725	15.631936	-0.127577	4.199173
665.720239	6033.105868	15.636941	-0.127575	4.196476
665.694072	6025.024528	15.641946	-0.127565	4.193736
665.516706	6017.027955	15.646951	-0.127526	4.191021
665.728466	6008.963150	15.651955	-0.127561	4.188286
666.087917	6000.977654	15.656960	-0.127622	4.185577
666.080330	5992.977284	15.661965	-0.127616	4.182857
665.836620	5985.043260	15.666970	-0.127565	4.180156
665.841981	5977.085902	15.671975	-0.127561	4.177448
665.406868	5969.061592	15.676979	-0.127475	4.174710
665.038560	5961.097231	15.681984	-0.127401	4.171991
665.243815	5953.019713	15.686989	-0.127434	4.169239
665.421213	5945.027064	15.691994	-0.127462	4.166513
665.357024	5937.000434	15.696999	-0.127445	4.163771
665.233180	5929.071626	15.702003	-0.127416	4.161060
665.305367	5921.063585	15.707008	-0.127425	4.158323
665.444865	5913.045651	15.712013	-0.127445	4.155581
665.490154	5904.998016	15.717018	-0.127448	4.152827
665.373809	5897.067140	15.722023	-0.127422	4.150108
665.543127	5889.002919	15.727027	-0.127448	4.147345
664.899216	5881.052469	15.732032	-0.127323	4.144610
665.070317	5873.122550	15.737037	-0.127350	4.141890
665.301085	5865.031163	15.742042	-0.127387	4.139113
664.963997	5857.129341	15.747047	-0.127319	4.136392
664.505641	5849.083996	15.752051	-0.127229	4.133619
664.930568	5841.104030	15.757056	-0.127303	4.130878
664.820295	5833.070281	15.762061	-0.127277	4.128109
664.832015	5824.987611	15.767066	-0.127274	4.125323
665.260192	5817.067572	15.772071	-0.127348	4.122597
664.871567	5809.069537	15.777075	-0.127271	4.119832
664.505645	5801.171966	15.782080	-0.127197	4.117099
664.461921	5793.076950	15.787085	-0.127184	4.114301
664.163901	5785.150640	15.792090	-0.127123	4.111556
664.622039	5777.053588	15.797095	-0.127203	4.108760
664.193721	5769.063824	15.802099	-0.127119	4.105987
664.692189	5761.030921	15.807104	-0.127206	4.103210
664.531989	5753.100150	15.812109	-0.127171	4.100458
664.310281	5745.092655	15.817114	-0.127125	4.097676
664.760341	5737.057840	15.822119	-0.127203	4.094892
664.880175	5729.059396	15.827123	-0.127220	4.092114
664.740691	5721.047975	15.832128	-0.127189	4.089327
664.915424	5713.038442	15.837133	-0.127216	4.086542
664.467283	5705.068382	15.842138	-0.127128	4.083761
664.759556	5697.129481	15.847143	-0.127177	4.080999
664.461206	5689.073089	15.852147	-0.127116	4.078186
664.303198	5681.129351	15.857152	-0.127082	4.075412
664.610770	5673.070952	15.862157	-0.127134	4.072603
664.703099	5665.026880	15.867162	-0.127146	4.069793
664.744974	5657.101112	15.872167	-0.127148	4.067023
664.503099	5649.031997	15.877171	-0.127098	4.064196
664.446136	5641.111508	15.882176	-0.127082	4.061422
663.697786	5633.164976	15.887181	-0.126938	4.058627
663.784472	5625.131082	15.892186	-0.126949	4.055812
663.637288	5617.149140	15.897191	-0.126916	4.053009
663.694862	5609.064493	15.902195	-0.126921	4.050172
663.784213	5601.092507	15.907200	-0.126933	4.047372
663.461576	5593.118886	15.912205	-0.126868	4.044564
663.136498	5585.153712	15.917210	-0.126802	4.041757
663.055219	5577.144623	15.922215	-0.126781	4.038936
663.079475	5569.133022	15.927219	-0.126781	4.036113
663.017790	5561.109544	15.932224	-0.126764	4.033283
662.845034	5553.053277	15.937229	-0.126727	4.030438
663.155491	5544.993786	15.942234	-0.126779	4.027598
663.221025	5537.000202	15.947239	-0.126786	4.024774
662.813102	5529.081874	15.952243	-0.126705	4.021968
663.164925	5521.030246	15.957248	-0.126765	4.019125
662.879885	5513.108028	15.962253	-0.126707	4.016316
662.855260	5505.035255	15.967258	-0.126697	4.013455
663.114644	5497.061870	15.972263	-0.126740	4.010632
663.127806	5489.046288	15.977267	-0.126738	4.007788
662.782248	5481.079185	15.982272	-0.126668	4.004954
662.500407	5473.141296	15.987277	-0.126610	4.002129
662.445826	5465.094200	15.992282	-0.126595	3.999266
661.945499	5457.258621	15.997287	-0.126497	3.996470
661.721488	5449.175734	16.002291	-0.126450	3.993588
661.843112	5441.159696	16.007296	-0.126467	3.990734
661.736455	5433.140812	16.012301	-0.126442	3.987872
661.499284	5425.105028	16.017306	-0.126393	3.985001
661.895647	5417.112448	16.022311	-0.126461	3.982153
662.242089	5409.041342	16.027315	-0.126521	3.979275
662.483787	5401.061221	16.032320	-0.126560	3.976425
662.624765	5393.069750	16.037325	-0.126581	3.973567
662.251306	5385.079966	16.042330	-0.126507	3.970699
662.086235	5377.163554	16.047335	-0.126471	3.967859
661.565998	5369.163083	16.052339	-0.126369	3.964981
662.170340	5361.120848	16.057344	-0.126476	3.962105
662.206012	5353.096363	16.062349	-0.126477	3.959223
661.840551	5345.186829	16.067354	-0.126404	3.956374
661.525663	5337.214724	16.072359	-0.126340	3.953501
661.465637	5329.121506	16.077363	-0.126324	3.950586
661.644577	5321.107326	16.082368	-0.126352	3.947702
661.699917	5313.092111	16.087373	-0.126357	3.944814
661.402849	5305.178244	16.092378	-0.126297	3.941954
661.517559	5297.132001	16.097383	-0.126313	3.939051
661.096649	5289.196406	16.102387	-0.126229	3.936176
661.208719	5281.125869	16.107392	-0.126245	3.933260
661.658327	5273.085520	16.112397	-0.126323	3.930359
661.383329	5265.108581	16.117402	-0.126267	3.927466
661.022409	5257.189414	16.122407	-0.126195	3.924589
661.552782	5249.097854	16.127411	-0.126288	3.921665
661.559149	5241.122571	16.132416	-0.126284	3.918771
661.198973	5233.215137	16.137421	-0.126212	3.915892
660.801995	5225.193657	16.142426	-0.126133	3.912970
660.858609	5217.203582	16.147431	-0.126138	3.910065
660.727817	5209.164082	16.152435	-0.126108	3.907136
660.965222	5201.107886	16.157440	-0.126147	3.904206
661.113285	5193.172799	16.162445	-0.126170	3.901316
660.727344	5185.141785	16.167450	-0.126093	3.898379
660.648544	5177.187861	16.172455	-0.126073	3.895474
660.449385	5169.189957	16.177459	-0.126031	3.892548
660.771824	5161.105356	16.182464	-0.126085	3.889598
660.871502	5153.147048	16.187469	-0.126099	3.886688
660.676127	5145.161148	16.192474	-0.126057	3.883760
661.020523	5137.195574	16.197479	-0.126116	3.880848
660.526887	5129.214990	16.202483	-0.126019	3.877911
660.642792	5121.186178	16.207488	-0.126035	3.874967
660.898124	5113.052985	16.212493	-0.126078	3.871985
660.865478	5105.011388	16.217498	-0.126066	3.869028
660.848611	5097.102347	16.222503	-0.126058	3.866118
660.280463	5089.167875	16.227507	-0.125947	3.863186
660.279356	5081.187033	16.232512	-0.125942	3.860246
660.238210	5073.208584	16.237517	-0.125929	3.857303
660.190438	5065.162188	16.242522	-0.125915	3.854333
660.267913	5057.245149	16.247527	-0.125924	3.851411
659.725871	5049.276902	16.252531	-0.125818	3.848455
659.965659	5041.153578	16.257536	-0.125857	3.845456
660.205502	5033.194166	16.262541	-0.125897	3.842515
659.746885	5025.238335	16.267546	-0.125806	3.839558
659.545572	5017.317094	16.272551	-0.125763	3.836618
659.447063	5009.260697	16.277555	-0.125740	3.833627
659.180639	5001.304338	16.282560	-0.125685	3.830667
659.025942	4993.268019	16.287565	-0.125651	3.827678
659.009988	4985.172961	16.292570	-0.125643	3.824667
658.849204	4977.288922	16.297575	-0.125608	3.821730
659.063040	4969.230002	16.302579	-0.125642	3.818733
658.756392	4961.268848	16.307584	-0.125580	3.815759
658.768060	4953.246023	16.312589	-0.125577	3.812767
659.111362	4945.159002	16.317594	-0.125635	3.809755
659.440280	4937.199366	16.322599	-0.125692	3.806789
659.046938	4929.216770	16.327603	-0.125613	3.803795
659.396366	4921.250735	16.332608	-0.125673	3.800822
659.234603	4913.302077	16.337613	-0.125638	3.797842
658.309592	4905.364556	16.342618	-0.125460	3.794846
658.655091	4897.308432	16.347623	-0.125519	3.791832
658.878181	4889.210233	16.352627	-0.125556	3.788798
658.878426	4881.217443	16.357632	-0.125550	3.785795
658.754128	4873.253484	16.362637	-0.125522	3.782798
658.394745	4865.299395	16.367642	-0.125450	3.779796
658.564101	4857.283931	16.372647	-0.125476	3.776782
658.207883	4849.308586	16.377651	-0.125405	3.773768
658.649988	4841.226278	16.382656	-0.125482	3.770730
658.444173	4833.258778	16.387661	-0.125438	3.767717
658.523111	4825.238042	16.392666	-0.125448	3.764689
658.523626	4817.302873	16.397671	-0.125443	3.761689
658.645849	4809.280710	16.402675	-0.125460	3.758656
658.491553	4801.279730	16.407680	-0.125426	3.755622
658.266269	4793.350656	16.412685	-0.125379	3.752612
658.255723	4785.327380	16.417690	-0.125372	3.749568
658.130378	4777.363060	16.422695	-0.125343	3.746542
657.374142	4769.408894	16.427699	-0.125197	3.743501
657.427370	4761.368454	16.432704	-0.125202	3.740445
657.767045	4753.374610	16.437709	-0.125260	3.737411
657.384817	4745.345401	16.442714	-0.125184	3.734344
657.708210	4737.347493	16.447719	-0.125239	3.731303
657.997087	4729.241202	16.452723	-0.125287	3.728218
657.807098	4721.303042	16.457728	-0.125247	3.725182
657.780742	4713.380497	16.462733	-0.125237	3.722154
657.509024	4705.394595	16.467738	-0.125181	3.719093
657.312426	4697.458627	16.472743	-0.125139	3.716051
657.054843	4689.401244	16.477747	-0.125086	3.712958
657.021944	4681.357204	16.482752	-0.125075	3.709873
657.162232	4673.353278	16.487757	-0.125095	3.706805
656.837465	4665.344178	16.492762	-0.125030	3.703721
656.989027	4657.382817	16.497767	-0.125053	3.700665
657.053256	4649.342873	16.502771	-0.125060	3.697574
657.122697	4641.340898	16.507776	-0.125067	3.694495
657.036154	4633.413429	16.512781	-0.125046	3.691439
656.888821	4625.354191	16.517786	-0.125013	3.688327
657.019418	4617.379486	16.522791	-0.125032	3.685252
656.626964	4609.427830	16.527795	-0.124954	3.682171
656.868703	4601.375842	16.532800	-0.124994	3.679064
657.036468	4593.410542	16.537805	-0.125020	3.675986
657.040569	4585.349277	16.542810	-0.125015	3.672864
657.054464	4577.378747	16.547815	-0.125013	3.669776
656.982319	4569.409511	16.552819	-0.124994	3.666682
656.610706	4561.446542	16.557824	-0.124920	3.663581
656.485529	4553.479272	16.562829	-0.124891	3.660482
656.386761	4545.481695	16.567834	-0.124868	3.657369
656.640746	4537.433866	16.572839	-0.124910	3.654243
656.426262	4529.428302	16.577843	-0.124865	3.651118
656.066155	4521.501385	16.582848	-0.124792	3.648018
656.534488	4513.410408	16.587853	-0.124874	3.644873
656.403945	4505.449325	16.592858	-0.124845	3.641760
656.510975	4497.471373	16.597863	-0.124860	3.638644
656.637501	4489.477315	16.602867	-0.124878	3.635520
655.884465	4481.581995	16.607872	-0.124733	3.632408
655.780437	4473.545466	16.612877	-0.124708	3.629255
655.608300	4465.536683	16.617882	-0.124671	3.626109
655.752078	4457.523740	16.622887	-0.124692	3.622967
655.736979	4449.498768	16.627891	-0.124684	3.619813
655.534031	4441.580637	16.632896	-0.124641	3.616693
655.982691	4433.466836	16.637901	-0.124720	3.613512
655.606776	4425.520274	16.642906	-0.124644	3.610371
655.462937	4417.570512	16.647911	-0.124612	3.607232
655.514588	4409.501419	16.652915	-0.124617	3.604049
655.859210	4401.516298	16.657920	-0.124676	3.600904
655.832343	4393.530099	16.662925	-0.124666	3.597746
655.722522	4385.546684	16.667930	-0.124640	3.594584
655.496374	4377.610313	16.672935	-0.124593	3.591434
655.389937	4369.573108	16.677939	-0.124568	3.588245
655.342589	4361.570250	16.682944	-0.124554	3.585068
655.504559	4353.569409	16.687949	-0.124578	3.581896
655.238971	4345.553575	16.692954	-0.124524	3.578702
655.039105	4337.638239	16.697959	-0.124481	3.575547
655.213676	4329.599697	16.702963	-0.124509	3.572351
655.180444	4321.575813	16.707968	-0.124497	3.569152
654.756349	4313.667142	16.712973	-0.124413	3.565985
654.517755	4305.663582	16.717978	-0.124364	3.562783
654.841833	4297.634757	16.722983	-0.124419	3.559584
654.505211	4289.704520	16.727987	-0.124351	3.556402
654.353162	4281.660137	16.732992	-0.124317	3.553177
655.071604	4273.503997	16.737997	-0.124446	3.549930
654.881642	4265.543243	16.743002	-0.124405	3.546732
654.984910	4257.547407	16.748007	-0.124419	3.543525
654.785145	4249.587923	16.753011	-0.124377	3.540321
654.590681	4241.626028	16.758016	-0.124335	3.537113
654.496611	4233.633575	16.763021	-0.124313	3.533893
654.527174	4225.661408	16.768026	-0.124313	3.530682
654.562147	4217.656681	16.773031	-0.124314	3.527455
654.157921	4209.685218	16.778035	-0.124234	3.524225
653.969396	4201.792725	16.783040	-0.124194	3.521031
654.346324	4193.724226	16.788045	-0.124259	3.517780
654.150165	4185.692649	16.793050	-0.124217	3.514523
654.112483	4177.742609	16.798055	-0.124205	3.511301
654.178342	4169.671025	16.803059	-0.124212	3.508030
654.256737	4161.655943	16.808064	-0.124221	3.504780
654.148879	4153.740385	16.813069	-0.124196	3.501560
653.598452	4145.787740	16.818074	-0.124088	3.498309
653.831219	4137.769053	16.823079	-0.124126	3.495053
653.525401	4129.795488	16.828083	-0.124064	3.491795
653.760620	4121.704983	16.833088	-0.124103	3.488503
654.163398	4113.676050	16.838093	-0.124172	3.485239
654.296837	4105.727733	16.843098	-0.124192	3.481996
653.954962	4097.786349	16.848103	-0.124123	3.478738
653.985166	4089.797030	16.853107	-0.124124	3.475469
653.965820	4081.817650	16.858112	-0.124115	3.472199
654.325457	4073.704386	16.863117	-0.124177	3.468884
653.758990	4065.798410	16.868122	-0.124066	3.465620
654.015530	4057.799063	16.873127	-0.124109	3.462342
653.671789	4049.806978	16.878131	-0.124039	3.459044
653.850916	4041.784243	16.883136	-0.124067	3.455748
653.768196	4033.842540	16.888141	-0.124047	3.452473
653.545793	4025.853924	16.893146	-0.124000	3.449170
653.310678	4017.904338	16.898151	-0.123951	3.445881
653.561356	4009.828450	16.903155	-0.123993	3.442552
653.815759	4001.796170	16.908160	-0.124035	3.439238
653.413732	3993.959457	16.913165	-0.123955	3.435980
653.552075	3985.882685	16.918170	-0.123975	3.432638
653.363475	3977.921876	16.923175	-0.123935	3.429329
653.555008	3969.887878	16.928179	-0.123966	3.426000
653.437508	3961.912689	16.933184	-0.123938	3.422681
653.405555	3953.927703	16.938189	-0.123927	3.419358
653.133855	3945.981659	16.943194	-0.123872	3.416040
653.467666	3937.881498	16.948199	-0.123928	3.412675
653.110569	3929.932853	16.953203	-0.123857	3.409346
652.729007	3922.027813	16.958208	-0.123781	3.406031
652.517273	3914.059682	16.963213	-0.123736	3.402692
652.346165	3906.011802	16.968218	-0.123699	3.399318
652.489049	3898.059514	16.973223	-0.123720	3.395992
652.608684	3889.953197	16.978227	-0.123737	3.392597
652.151995	3881.970636	16.983232	-0.123647	3.389230
651.787839	3874.062646	16.988237	-0.123574	3.385895
652.138328	3865.957915	16.993242	-0.123634	3.382499
652.338993	3857.964359	16.998247	-0.123666	3.379141
652.601806	3849.924478	17.003251	-0.123710	3.375762
652.639169	3841.940679	17.008256	-0.123712	3.372396
652.148259	3834.049337	17.013261	-0.123615	3.369046
652.440269	3825.990960	17.018266	-0.123664	3.365650
652.078624	3818.128940	17.023271	-0.123592	3.362311
652.080995	3810.082842	17.028275	-0.123587	3.358903
651.841855	3802.130594	17.033280	-0.123537	3.355523
652.208908	3794.069166	17.038285	-0.123600	3.352115
652.202696	3786.035008	17.043290	-0.123594	3.348702
652.122245	3778.103574	17.048295	-0.123574	3.345326
651.607821	3770.193912	17.053299	-0.123473	3.341940
651.454580	3762.175946	17.058304	-0.123439	3.338518
651.670389	3754.166813	17.063309	-0.123474	3.335109
651.623822	3746.135497	17.068314	-0.123460	3.331678
651.384220	3738.180597	17.073319	-0.123410	3.328269
651.425023	3730.142104	17.078323	-0.123413	3.324831
651.371004	3722.218654	17.083328	-0.123398	3.321435
651.354654	3714.206840	17.088333	-0.123389	3.318000
651.959259	3706.104502	17.093338	-0.123497	3.314545
651.500649	3698.236523	17.098343	-0.123406	3.311147
650.973114	3690.255309	17.103347	-0.123303	3.307694
651.336790	3682.185530	17.108352	-0.123365	3.304234
651.275553	3674.273640	17.113357	-0.123349	3.300821
651.152223	3666.257659	17.118362	-0.123320	3.297358
650.791978	3658.340140	17.123367	-0.123248	3.293924
650.971408	3650.245930	17.128371	-0.123276	3.290432
651.349672	3642.199918	17.133376	-0.123341	3.286964
650.964168	3634.283318	17.138381	-0.123265	3.283519
651.133469	3626.268692	17.143386	-0.123291	3.280050
651.163229	3618.331231	17.148391	-0.123291	3.276605
650.436152	3610.429526	17.153395	-0.123151	3.273141
650.318053	3602.386193	17.158400	-0.123123	3.269637
650.071619	3594.437090	17.163405	-0.123072	3.266165
650.331997	3586.344115	17.168410	-0.123116	3.262646
650.331071	3578.371716	17.173415	-0.123110	3.259166
649.941695	3570.483648	17.178419	-0.123033	3.255703
649.950482	3562.415436	17.183424	-0.123029	3.252174
650.309233	3554.375586	17.188429	-0.123091	3.248668
650.620237	3546.324475	17.193434	-0.123143	3.245151
650.574585	3538.421050	17.198439	-0.123130	3.241681
650.202908	3530.476239	17.203443	-0.123055	3.238175
650.002463	3522.501525	17.208448	-0.123013	3.234659
649.769621	3514.561291	17.213453	-0.122964	3.231154
649.680831	3506.497359	17.218458	-0.122942	3.227595
650.018005	3498.409410	17.223463	-0.123000	3.224040
650.241499	3490.435574	17.228467	-0.123036	3.220527
650.423491	3482.432620	17.233472	-0.123065	3.216996
650.198711	3474.479646	17.238477	-0.123018	3.213465
650.296872	3466.445793	17.243482	-0.123031	3.209909
650.539865	3458.469638	17.248487	-0.123071	3.206380
650.248412	3450.523484	17.253491	-0.123012	3.202838
649.813452	3442.590124	17.258496	-0.122925	3.199292
649.608109	3434.682394	17.263501	-0.122882	3.195762
649.560834	3426.613651	17.268506	-0.122868	3.192164
649.821239	3418.588161	17.273511	-0.122911	3.188595
649.501358	3410.620313	17.278515	-0.122846	3.185022
649.306860	3402.682985	17.283520	-0.122805	3.181464
649.266824	3394.686763	17.288525	-0.122792	3.177882
649.233924	3386.627879	17.293530	-0.122781	3.174269
649.651787	3378.630485	17.298535	-0.122854	3.170699
649.698504	3370.593875	17.303539	-0.122857	3.167091
649.606833	3362.634674	17.308544	-0.122835	3.163507
650.066037	3354.637092	17.313549	-0.122915	3.159927
649.681109	3346.735623	17.318554	-0.122838	3.156348
649.589183	3338.714382	17.323559	-0.122816	3.152724
649.293401	3330.762455	17.328563	-0.122756	3.149119
649.433245	3322.750778	17.333568	-0.122777	3.145501
649.193314	3314.800102	17.338573	-0.122727	3.141890
649.216492	3306.752214	17.343578	-0.122726	3.138243
649.737881	3298.712565	17.348583	-0.122818	3.134617
649.664416	3290.761455	17.353587	-0.122799	3.131001
649.109045	3282.844056	17.358592	-0.122690	3.127374
649.529862	3274.795935	17.363597	-0.122763	3.123728
649.111614	3266.908307	17.368602	-0.122680	3.120112
648.624910	3258.997907	17.373607	-0.122584	3.116479
648.369284	3250.995372	17.378611	-0.122532	3.112810
648.328410	3242.939299	17.383616	-0.122519	3.109121
648.106648	3234.977025	17.388621	-0.122472	3.105463
647.934443	3226.958044	17.393626	-0.122435	3.101777
648.204047	3218.953767	17.398631	-0.122480	3.098114
647.869307	3210.994724	17.403635	-0.122413	3.094439
648.014850	3202.971651	17.408640	-0.122434	3.090752
648.303402	3194.942909	17.413645	-0.122483	3.087066
648.326677	3186.957310	17.418650	-0.122482	3.083382
647.950638	3179.061038	17.423655	-0.122407	3.079716
647.563367	3171.125586	17.428659	-0.122330	3.076028
648.024128	3162.982546	17.433664	-0.122410	3.072279
647.676872	3155.066468	17.438669	-0.122340	3.068592
647.822025	3146.989970	17.443674	-0.122362	3.064849
648.024506	3139.031500	17.448679	-0.122395	3.061160
647.872113	3131.085510	17.453683	-0.122361	3.057455
647.764065	3123.104480	17.458688	-0.122336	3.053732
647.433530	3115.156889	17.463693	-0.122269	3.050008
647.459837	3107.128140	17.468698	-0.122269	3.046260
648.062480	3099.047514	17.473703	-0.122376	3.042510
648.108148	3091.101028	17.478707	-0.122379	3.038792
648.197640	3083.133728	17.483712	-0.122390	3.035061
647.825602	3075.232270	17.488717	-0.122316	3.031335
647.445289	3067.254611	17.493722	-0.122240	3.027567
647.691125	3059.214933	17.498727	-0.122280	3.023796
647.524412	3051.273440	17.503731	-0.122244	3.020047
647.456780	3043.287175	17.508736	-0.122226	3.016276
647.263144	3035.343348	17.513741	-0.122185	3.012515
647.456174	3027.285651	17.518746	-0.122216	3.008714
647.155939	3019.333620	17.523751	-0.122155	3.004934
647.590163	3011.317340	17.528755	-0.122230	3.001156
647.459776	3003.371431	17.533760	-0.122201	2.997377
647.307801	2995.395890	17.538765	-0.122168	2.993579
647.209498	2987.370424	17.543770	-0.122144	2.989755
647.146152	2979.432094	17.548775	-0.122127	2.985969
646.630613	2971.526640	17.553779	-0.122026	2.982171
646.466183	2963.516906	17.558784	-0.121990	2.978337
647.437427	2955.348916	17.563789	-0.122166	2.974479
647.136674	2947.440259	17.568794	-0.122104	2.970676
647.070862	2939.473031	17.573799	-0.122087	2.966852
646.846443	2931.521504	17.578803	-0.122040	2.963022
647.031636	2923.502424	17.583808	-0.122069	2.959176
646.874903	2915.598689	17.588813	-0.122035	2.955363
646.427089	2907.640332	17.593818	-0.121946	2.951503
646.784553	2899.563873	17.598823	-0.122008	2.947624
647.054821	2891.519602	17.603827	-0.122053	2.943750
646.897124	2883.607165	17.608832	-0.122018	2.939912
646.533254	2875.707033	17.613837	-0.121945	2.936065
646.688303	2867.647575	17.618842	-0.121969	2.932162
646.188824	2859.749404	17.623847	-0.121871	2.928298
646.179670	2851.687590	17.628851	-0.121864	2.924375
646.327881	2843.740346	17.633856	-0.121886	2.920511
646.198431	2835.796366	17.638861	-0.121857	2.916629
646.106331	2827.765027	17.643866	-0.121835	2.912701
646.236548	2819.719378	17.648871	-0.121854	2.908773
646.171099	2811.723377	17.653875	-0.121836	2.904853
646.338045	2803.737891	17.658880	-0.121862	2.900945
646.070639	2795.837348	17.663885	-0.121807	2.897050
645.714166	2787.875009	17.668890	-0.121736	2.893115
645.604536	2779.912030	17.673895	-0.121710	2.889188
645.690367	2771.883080	17.678899	-0.121721	2.885233
645.463170	2763.946844	17.683904	-0.121673	2.881302
645.466026	2755.986332	17.688909	-0.121669	2.877365
645.118172	2748.001714	17.693914	-0.121599	2.873392
644.868457	2740.061970	17.698919	-0.121547	2.869441
644.946791	2732.034161	17.703923	-0.121556	2.865460
645.082450	2724.005355	17.708928	-0.121576	2.861475
645.661982	2715.940646	17.713933	-0.121679	2.857492
645.501297	2707.983773	17.718938	-0.121644	2.853515
646.134024	2699.930644	17.723943	-0.121756	2.849530
645.586790	2692.068595	17.728947	-0.121649	2.845568
645.237810	2684.180912	17.733952	-0.121579	2.841599
645.475549	2676.164170	17.738957	-0.121618	2.837593
645.306677	2668.180795	17.743962	-0.121582	2.833574
645.420794	2660.169039	17.748967	-0.121598	2.829552
645.236958	2652.209548	17.753971	-0.121558	2.825534
645.430115	2644.205243	17.758976	-0.121589	2.821508
645.009558	2636.303778	17.763981	-0.121506	2.817494
645.292208	2628.224910	17.768986	-0.121553	2.813425
645.497242	2620.240441	17.773991	-0.121586	2.809393
645.362530	2612.302866	17.778995	-0.121556	2.805359
645.122075	2604.352159	17.784000	-0.121506	2.801307
645.457529	2596.336542	17.789005	-0.121563	2.797249
645.146458	2588.381687	17.794010	-0.121500	2.793179
644.656189	2580.486954	17.799015	-0.121403	2.789123
644.576063	2572.492705	17.804019	-0.121383	2.785034
644.569298	2564.496804	17.809024	-0.121377	2.780942
644.565447	2556.521465	17.814029	-0.121371	2.776856
644.547025	2548.532824	17.819034	-0.121362	2.772755
644.465944	2540.571853	17.824039	-0.121342	2.768659
644.419372	2532.556827	17.829043	-0.121328	2.764531
644.430821	2524.596603	17.834048	-0.121325	2.760429
644.883784	2516.570806	17.839053	-0.121404	2.756313
644.667866	2508.585585	17.844058	-0.121359	2.752172
644.776309	2500.563319	17.849063	-0.121374	2.748025
644.792220	2492.585713	17.854067	-0.121372	2.743889
644.850841	2484.621066	17.859072	-0.121377	2.739757
644.622086	2476.710934	17.864077	-0.121330	2.735629
644.312754	2468.767956	17.869082	-0.121267	2.731472
644.420289	2460.765440	17.874087	-0.121282	2.727304
644.496582	2452.781810	17.879091	-0.121291	2.723137
644.214103	2444.846688	17.884096	-0.121233	2.718967
644.079051	2436.916364	17.889101	-0.121203	2.714802
644.030428	2428.918382	17.894106	-0.121188	2.710601
644.001321	2420.943536	17.899111	-0.121178	2.706407
643.835904	2412.976141	17.904115	-0.121142	2.702201
643.745982	2405.010961	17.909120	-0.121120	2.697995
643.694887	2397.015765	17.914125	-0.121105	2.693768
643.845771	2388.978647	17.919130	-0.121128	2.689526
644.028330	2381.023290	17.924135	-0.121157	2.685323
643.889289	2373.079906	17.929139	-0.121126	2.681098
643.122644	2365.240627	17.934144	-0.120978	2.676882
643.698598	2357.135329	17.939149	-0.121080	2.672604
643.285075	2349.200123	17.944154	-0.120998	2.668346
643.503883	2341.142805	17.949159	-0.121033	2.664057
642.902422	2333.294844	17.954163	-0.120916	2.659820
643.267607	2325.242966	17.959168	-0.120979	2.655530
643.336748	2317.251819	17.964173	-0.120986	2.651246
643.206896	2309.272746	17.969178	-0.120957	2.646948
643.271188	2301.319897	17.974183	-0.120964	2.642670
643.271217	2293.343842	17.979187	-0.120959	2.638369
642.636871	2285.475260	17.984192	-0.120835	2.634076
642.985135	2277.422585	17.989197	-0.120895	2.629743
642.654338	2269.489501	17.994202	-0.120828	2.625421
642.531710	2261.542706	17.999207	-0.120800	2.621099
642.566091	2253.542544	18.004211	-0.120801	2.616751
642.923089	2245.494329	18.009216	-0.120863	2.612392
642.807519	2237.551945	18.014221	-0.120836	2.608051
642.472187	2229.612310	18.019226	-0.120768	2.603690
642.211166	2221.729031	18.024231	-0.120715	2.599357
642.346533	2213.723810	18.029235	-0.120735	2.594977
641.986999	2205.662868	18.034240	-0.120662	2.590525
642.425144	2197.589260	18.039245	-0.120739	2.586113
642.590602	2189.624581	18.044250	-0.120764	2.581735
642.697827	2181.665951	18.049255	-0.120779	2.577349
642.093980	2173.796110	18.054259	-0.120661	2.572955
642.480758	2165.757485	18.059264	-0.120728	2.568529
642.560360	2157.786521	18.064269	-0.120738	2.564111
642.206470	2149.909706	18.069274	-0.120667	2.559708
642.011544	2141.989785	18.074279	-0.120625	2.555284
642.088005	2133.988241	18.079283	-0.120634	2.550827
641.581019	2126.079371	18.084288	-0.120535	2.546371
641.340829	2118.142552	18.089293	-0.120485	2.541912
641.308457	2110.142368	18.094298	-0.120474	2.537423
641.780628	2102.062956	18.099303	-0.120556	2.532919
641.767235	2094.089465	18.104307	-0.120549	2.528431
641.450560	2086.178718	18.109312	-0.120485	2.523948
641.204350	2078.285311	18.114317	-0.120434	2.519473
641.581748	2070.217231	18.119322	-0.120499	2.514936
641.470322	2062.273233	18.124327	-0.120473	2.510425
641.432129	2054.289628	18.129331	-0.120460	2.505889
640.940447	2046.394455	18.134336	-0.120364	2.501362
641.072093	2038.419513	18.139341	-0.120383	2.496828
641.004082	2030.436772	18.144346	-0.120365	2.492265
641.250519	2022.419683	18.149351	-0.120406	2.487698
640.817309	2014.525385	18.154355	-0.120320	2.483143
641.585263	2006.429946	18.159360	-0.120458	2.478553
641.127205	1998.598639	18.164365	-0.120367	2.474015
640.552186	1990.696021	18.169370	-0.120255	2.469418
640.744326	1982.683286	18.174375	-0.120286	2.464807
640.588995	1974.753308	18.179379	-0.120252	2.460209
640.499610	1966.769574	18.184384	-0.120230	2.455576
640.523062	1958.793117	18.189389	-0.120229	2.450948
640.220281	1950.849956	18.194394	-0.120167	2.446305
640.556342	1942.840569	18.199399	-0.120225	2.441663
640.533227	1934.875149	18.204403	-0.120215	2.437011
640.745703	1926.860490	18.209408	-0.120250	2.432339
641.004903	1918.864748	18.214413	-0.120293	2.427673
640.425491	1910.989761	18.219418	-0.120180	2.423004
640.066001	1903.095828	18.224423	-0.120108	2.418332
640.248388	1895.085037	18.229427	-0.120136	2.413624
640.195800	1887.097261	18.234432	-0.120121	2.408902
640.305732	1879.128544	18.239437	-0.120137	2.404194
639.788431	1871.277228	18.244442	-0.120035	2.399498
640.316640	1863.220476	18.249447	-0.120128	2.394753
639.807324	1855.363293	18.254451	-0.120028	2.390035
639.745375	1847.370465	18.259456	-0.120012	2.385263
639.721038	1839.424882	18.264461	-0.120002	2.380512
639.706642	1831.423526	18.269466	-0.119994	2.375719
639.720637	1823.469315	18.274471	-0.119991	2.370946
640.170205	1815.425426	18.279475	-0.120070	2.366146
640.124963	1807.494652	18.284480	-0.120056	2.361364
639.921810	1799.619914	18.289485	-0.120013	2.356593
639.479510	1791.702897	18.294490	-0.119926	2.351767
639.588325	1783.723818	18.299495	-0.119941	2.346939
638.875057	1775.873746	18.304499	-0.119803	2.342112
638.733204	1767.895495	18.309504	-0.119771	2.337243
638.719425	1759.927501	18.314509	-0.119764	2.332381
638.715786	1751.906625	18.319514	-0.119758	2.327478
639.098942	1743.870178	18.324519	-0.119824	2.322587
639.131073	1735.959112	18.329523	-0.119825	2.317733
638.783844	1728.050130	18.334528	-0.119755	2.312839
638.997740	1720.049024	18.339533	-0.119789	2.307924
638.806474	1712.116415	18.344538	-0.119749	2.303008
638.675767	1704.217217	18.349543	-0.119719	2.298106
638.485486	1696.257703	18.354547	-0.119678	2.293151
638.369603	1688.299729	18.359552	-0.119652	2.288193
638.266595	1680.375808	18.364557	-0.119627	2.283247
638.011164	1672.467478	18.369562	-0.119575	2.278286
637.673768	1664.533574	18.374567	-0.119507	2.273291
638.152340	1656.421863	18.379571	-0.119591	2.268245
637.704102	1648.539436	18.384576	-0.119502	2.263251
637.888352	1640.550101	18.389581	-0.119531	2.258233
638.028471	1632.549708	18.394586	-0.119552	2.253194
637.821199	1624.669268	18.399591	-0.119508	2.248189
637.719422	1616.722938	18.404595	-0.119484	2.243140
637.845540	1608.755569	18.409600	-0.119502	2.238086
637.963188	1600.812908	18.414605	-0.119519	2.233036
638.143450	1592.810234	18.419610	-0.119547	2.227942
637.640571	1584.970385	18.424615	-0.119449	2.222879
637.339093	1577.059162	18.429619	-0.119387	2.217777
637.651852	1569.030617	18.434624	-0.119440	2.212643
637.592076	1561.105420	18.439629	-0.119424	2.207530
637.600688	1553.132474	18.444634	-0.119421	2.202380
637.691946	1545.199456	18.449639	-0.119432	2.197252
637.782719	1537.240502	18.454643	-0.119444	2.192095
637.450173	1529.328342	18.459648	-0.119377	2.186917
637.318437	1521.408783	18.464653	-0.119347	2.181740
637.929819	1513.346150	18.469658	-0.119456	2.176527
637.672595	1505.471010	18.474663	-0.119403	2.171343
637.684410	1497.510734	18.479667	-0.119400	2.166116
637.152862	1489.688181	18.484672	-0.119296	2.160916
637.102889	1481.761652	18.489677	-0.119281	2.155680
636.748406	1473.844726	18.494682	-0.119210	2.150409
636.790707	1465.872011	18.499687	-0.119213	2.145126
637.190037	1457.855216	18.504691	-0.119282	2.139834
636.220271	1450.084645	18.509696	-0.119096	2.134562
636.646238	1442.047237	18.514701	-0.119170	2.129233
635.991650	1434.183465	18.519706	-0.119043	2.123902
636.268570	1426.199686	18.524711	-0.119090	2.118568
636.330134	1418.217808	18.529715	-0.119096	2.113200
636.484092	1410.215519	18.534720	-0.119120	2.107815
636.091570	1402.342901	18.539725	-0.119041	2.102449
636.022372	1394.400086	18.544730	-0.119023	2.097054
635.903051	1386.496255	18.549735	-0.118996	2.091666
636.034108	1378.495048	18.554739	-0.119015	2.086223
635.290521	1370.699225	18.559744	-0.118872	2.080820
635.707430	1362.690133	18.564749	-0.118944	2.075371
635.953829	1354.683987	18.569754	-0.118985	2.069893
635.983187	1346.756574	18.574759	-0.118985	2.064434
635.635577	1338.896707	18.579763	-0.118915	2.058968
635.782536	1330.933016	18.584768	-0.118937	2.053466
635.643628	1323.026438	18.589773	-0.118906	2.047960
635.169840	1315.168499	18.594778	-0.118813	2.042438
635.307630	1307.204640	18.599783	-0.118833	2.036890
635.265980	1299.280555	18.604787	-0.118820	2.031337
635.062121	1291.338152	18.609792	-0.118777	2.025738
635.099098	1283.404614	18.614797	-0.118779	2.020155
635.242446	1275.439684	18.619802	-0.118801	2.014546
635.024862	1267.556213	18.624807	-0.118755	2.008941
634.971057	1259.631739	18.629811	-0.118740	2.003308
635.034952	1251.702455	18.634816	-0.118746	1.997669
635.580126	1243.693562	18.639821	-0.118843	1.992007
634.830179	1235.888737	18.644826	-0.118698	1.986338
635.120384	1227.911956	18.649831	-0.118747	1.980640
634.869505	1220.050120	18.654835	-0.118695	1.974951
634.963329	1212.072836	18.659840	-0.118707	1.969199
635.016299	1204.165750	18.664845	-0.118712	1.963476
634.658762	1196.312920	18.669850	-0.118640	1.957731
634.098476	1188.497361	18.674855	-0.118531	1.951975
633.816893	1180.560623	18.679859	-0.118473	1.946143
633.856267	1172.601076	18.684864	-0.118475	1.940312
634.168232	1164.604823	18.689869	-0.118528	1.934467
634.009819	1156.687124	18.694874	-0.118494	1.928610
634.071224	1148.765646	18.699879	-0.118500	1.922756
634.221444	1140.828308	18.704883	-0.118523	1.916883
633.743585	1132.995788	18.709888	-0.118429	1.911000
633.762099	1125.067835	18.714893	-0.118427	1.905082
633.622220	1117.169154	18.719898	-0.118396	1.899151
633.650772	1109.247645	18.724903	-0.118396	1.893203
633.585540	1101.324505	18.729907	-0.118379	1.887224
633.865001	1093.378300	18.734912	-0.118425	1.881248
633.287098	1085.596090	18.739917	-0.118313	1.875279
633.161214	1077.666231	18.744922	-0.118284	1.869230
633.214618	1069.725092	18.749927	-0.118289	1.863174
633.382872	1061.784975	18.754931	-0.118315	1.857113
632.975552	1053.948711	18.759936	-0.118234	1.851044
633.373771	1045.949902	18.764941	-0.118303	1.844924
633.057571	1038.127959	18.769946	-0.118239	1.838837
633.176649	1030.195884	18.774951	-0.118256	1.832695
633.091516	1022.299704	18.779955	-0.118235	1.826537
632.815077	1014.435374	18.784960	-0.118179	1.820359
632.854397	1006.550956	18.789965	-0.118181	1.814183
632.274445	998.725509	18.794970	-0.118068	1.807956
632.473759	990.788459	18.799975	-0.118100	1.801715
632.773788	982.834147	18.804979	-0.118150	1.795452
632.637333	974.915638	18.809984	-0.118120	1.789140
632.712214	967.006167	18.814989	-0.118128	1.782840
632.290730	959.189722	18.819994	-0.118045	1.776531
632.343035	951.278104	18.824999	-0.118049	1.770181
632.297038	943.383250	18.830003	-0.118036	1.763810
632.425748	935.483655	18.835008	-0.118055	1.757434
632.171285	927.657714	18.840013	-0.118002	1.751046
631.781013	919.801124	18.845018	-0.117924	1.744592
631.888000	911.895205	18.850023	-0.117939	1.738137
631.782397	904.024169	18.855027	-0.117914	1.731660
631.787230	896.112917	18.860032	-0.117910	1.725139
631.704171	888.283009	18.865037	-0.117889	1.718650
631.655447	880.388750	18.870042	-0.117875	1.712087
631.352056	872.544930	18.875047	-0.117814	1.705507
631.146662	864.696789	18.880051	-0.117770	1.698911
631.029542	856.822855	18.885056	-0.117743	1.692279
631.135197	848.923522	18.890061	-0.117758	1.685630
630.871993	841.079998	18.895066	-0.117704	1.678952
630.704609	833.240221	18.900071	-0.117668	1.672263
630.693579	825.340289	18.905075	-0.117660	1.665517
630.701068	817.463368	18.910080	-0.117657	1.658766
630.619653	809.598033	18.915085	-0.117636	1.651985
630.540424	801.721583	18.920090	-0.117616	1.645167
630.753366	793.858259	18.925095	-0.117651	1.638372
630.541993	786.011793	18.930099	-0.117606	1.631505
630.080187	778.188580	18.935104	-0.117515	1.624594
630.358070	770.274179	18.940109	-0.117562	1.617677
630.214875	762.424632	18.945114	-0.117530	1.610728
630.134209	754.584764	18.950119	-0.117510	1.603767
630.243457	746.721472	18.955123	-0.117525	1.596781
630.355556	738.837247	18.960128	-0.117541	1.589747
630.477105	730.977700	18.965133	-0.117559	1.582705
630.183973	723.196882	18.970138	-0.117499	1.575642
630.197930	715.358277	18.975143	-0.117496	1.568540
630.276351	707.500176	18.980147	-0.117506	1.561397
629.910530	699.738735	18.985152	-0.117433	1.554244
630.100575	691.860180	18.990157	-0.117463	1.547033
629.990742	684.029959	18.995162	-0.117437	1.539788
629.583017	676.279668	19.000167	-0.117356	1.532538
629.488033	668.443529	19.005171	-0.117334	1.525220
629.378217	660.638285	19.010176	-0.117308	1.517894
629.051197	652.868781	19.015181	-0.117242	1.510533
629.450666	644.917224	19.020186	-0.117311	1.503076
629.338565	637.136023	19.025191	-0.117285	1.495664
629.593044	629.261704	19.030195	-0.117328	1.488183
629.093973	621.546301	19.035200	-0.117230	1.480699
629.408007	613.692492	19.040205	-0.117283	1.473171
629.242277	605.859344	19.045210	-0.117247	1.465549
628.891158	598.133781	19.050215	-0.117177	1.457962
628.731792	590.338705	19.055219	-0.117142	1.450298
628.250778	582.614378	19.060224	-0.117047	1.442611
628.496073	574.759076	19.065229	-0.117088	1.434871
629.096827	566.828707	19.070234	-0.117195	1.427073
628.873244	559.102448	19.075239	-0.117148	1.419301
628.665231	551.358735	19.080243	-0.117104	1.411470
627.892759	543.702024	19.085248	-0.116955	1.403589
627.660605	535.969431	19.090253	-0.116907	1.395678
627.655393	528.143744	19.095258	-0.116901	1.387664
627.456714	520.383069	19.100263	-0.116859	1.379638
627.306167	512.613097	19.105267	-0.116826	1.371563
626.735858	504.921872	19.110272	-0.116715	1.363449
626.150572	497.258038	19.115277	-0.116601	1.355313
625.850906	489.487516	19.120282	-0.116540	1.347065
625.425445	481.774528	19.125287	-0.116456	1.338805
625.301446	473.979610	19.130291	-0.116427	1.330460
624.668461	466.306047	19.135296	-0.116305	1.322101
623.882708	458.656242	19.140301	-0.116153	1.313687
623.359476	450.852920	19.145306	-0.116051	1.305098
622.399495	443.235878	19.150311	-0.115867	1.296577
621.203004	435.631196	19.155315	-0.115639	1.287968
620.005130	428.017628	19.160320	-0.115411	1.279290
619.283938	420.320551	19.165325	-0.115272	1.270550
618.215930	412.669486	19.170330	-0.115068	1.261734
617.095694	405.059625	19.175335	-0.114855	1.252892
616.335118	397.357561	19.180339	-0.114708	1.243952
615.849240	389.630414	19.185344	-0.114612	1.234971
614.754874	382.024713	19.190349	-0.114404	1.225945
614.012620	374.342204	19.195354	-0.114261	1.216832
613.758891	366.576304	19.200359	-0.114208	1.207649
612.907943	358.960462	19.205363	-0.114045	1.198454
611.938032	351.366011	19.210368	-0.113859	1.189188
611.617571	343.653629	19.215373	-0.113795	1.179841
610.665090	336.064505	19.220378	-0.113612	1.170437
609.855788	328.466318	19.225383	-0.113457	1.160975
609.156185	320.843739	19.230387	-0.113321	1.151429
608.567410	313.173471	19.235392	-0.113207	1.141767
607.971018	305.568988	19.240397	-0.113091	1.132103
607.409868	297.940380	19.245402	-0.112981	1.122332
606.525618	290.407957	19.250407	-0.112812	1.112528
605.195232	282.944224	19.255411	-0.112559	1.102625
604.258492	275.408540	19.260416	-0.112380	1.092627
604.005140	267.759348	19.265421	-0.112328	1.082541
603.102632	260.263776	19.270426	-0.112155	1.072416
602.189991	252.759228	19.275431	-0.111980	1.062179
601.931345	245.140296	19.280435	-0.111927	1.051841
601.026733	237.662063	19.285440	-0.111754	1.041440
600.443727	230.155283	19.290445	-0.111640	1.030970
599.149924	222.763280	19.295450	-0.111394	1.020381
598.488964	215.282916	19.300455	-0.111266	1.009711
597.753486	207.820270	19.305459	-0.111125	0.998933
597.295699	200.300948	19.310464	-0.111034	0.988025
596.237600	192.932269	19.315469	-0.110833	0.977062
595.788159	185.438813	19.320474	-0.110744	0.965947
594.774137	178.096957	19.325479	-0.110550	0.954781
594.072580	170.703296	19.330483	-0.110415	0.943487
593.779584	163.242712	19.335488	-0.110356	0.932062
592.933713	155.927944	19.340493	-0.110193	0.920572
592.012317	148.634204	19.345498	-0.110017	0.908948
590.934162	141.381961	19.350503	-0.109812	0.897195
590.528901	134.020375	19.355507	-0.109731	0.885300
589.528117	126.803273	19.360512	-0.109540	0.873307
588.551828	119.594128	19.365517	-0.109354	0.861167
588.019868	112.323199	19.370522	-0.109250	0.848881
587.366842	105.105884	19.375527	-0.109124	0.836468
586.454814	97.950024	19.380531	-0.108949	0.823896
585.355979	90.857653	19.385536	-0.108740	0.811182
584.835929	83.687223	19.390541	-0.108638	0.798308
583.943772	76.617693	19.395546	-0.108468	0.785286
582.968031	69.790687	19.400551	-0.108282	0.772465