Mon Apr 19 10:01:30 2021

Number of Points = 3640
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.017601	-0.065033	0.000000	-0.000066	0.310238

1.970604	-0.061566	0.005005	-0.000057	0.310214
1.707330	-0.013810	0.010010	-0.000008	0.310214
2.168263	-0.100985	0.015014	-0.000094	0.310198
1.976168	-0.062040	0.020019	-0.000058	0.310217
1.959848	-0.061837	0.025024	-0.000055	0.310204
2.433965	-0.148746	0.030029	-0.000143	0.310200
2.180957	-0.101914	0.035034	-0.000096	0.310204
1.700159	-0.011407	0.040038	-0.000007	0.310218
1.762018	-0.021371	0.045043	-0.000018	0.310224
1.989206	-0.066313	0.050048	-0.000061	0.310207
2.295725	-0.122936	0.055053	-0.000118	0.310203
2.343591	-0.134093	0.060058	-0.000126	0.310191
2.116569	-0.153635	0.065062	-0.000084	0.309907
2.449288	-0.218554	0.070067	-0.000146	0.309887
2.184571	-0.172006	0.075072	-0.000097	0.309879
1.859024	-0.107827	0.080077	-0.000036	0.309903
2.393103	-0.209940	0.085082	-0.000136	0.309879
2.335267	-0.198881	0.090086	-0.000125	0.309881
1.912404	-0.186300	0.095091	-0.000046	0.309581
1.679491	-0.146973	0.100096	-0.000003	0.309567
2.615703	-0.322732	0.105101	-0.000177	0.309541
2.381388	-0.279648	0.110106	-0.000133	0.309543
1.973597	-0.203947	0.115110	-0.000057	0.309550
2.185203	-0.299168	0.120115	-0.000097	0.309285
2.192750	-0.304356	0.125120	-0.000098	0.309267
2.085320	-0.282069	0.130125	-0.000078	0.309280
2.296094	-0.321299	0.135130	-0.000117	0.309275
2.256814	-0.383363	0.140134	-0.000110	0.308951
1.842955	-0.308553	0.145139	-0.000033	0.308949
1.908027	-0.323427	0.150144	-0.000045	0.308935
2.001094	-0.351648	0.155149	-0.000062	0.308882
1.813027	-0.372673	0.160154	-0.000027	0.308623
1.246256	-0.264573	0.165158	0.000078	0.308647
1.537655	-0.316715	0.170163	0.000024	0.308651
1.804542	-0.403230	0.175168	-0.000026	0.308473
1.777488	-0.429372	0.180173	-0.000020	0.308327
1.349583	-0.351538	0.185178	0.000059	0.308327
1.386146	-0.366614	0.190182	0.000052	0.308288
1.056539	-0.356792	0.195187	0.000114	0.308052
1.355652	-0.414164	0.200192	0.000058	0.308038
1.612316	-0.459898	0.205197	0.000010	0.308042
1.782925	-0.556210	0.210202	-0.000021	0.307735
1.609482	-0.533810	0.215206	0.000011	0.307692
1.836363	-0.580670	0.220211	-0.000031	0.307666
1.822882	-0.641249	0.225216	-0.000029	0.307369
1.807810	-0.636168	0.230221	-0.000026	0.307380
1.714578	-0.654552	0.235226	-0.000008	0.307214
1.413459	-0.632745	0.240230	0.000048	0.307059
1.367634	-0.623210	0.245235	0.000056	0.307064
2.027225	-0.804759	0.250240	-0.000066	0.306773
1.389282	-0.687748	0.255245	0.000052	0.306778
1.149632	-0.679308	0.260250	0.000097	0.306613
1.149029	-0.713970	0.265254	0.000097	0.306449
1.266626	-0.737388	0.270259	0.000075	0.306439
0.947094	-0.740960	0.275264	0.000135	0.306148
1.139075	-0.775725	0.280269	0.000099	0.306148
1.191246	-0.828251	0.285274	0.000089	0.305944
1.512765	-0.915582	0.290278	0.000030	0.305808
1.522294	-0.940835	0.295283	0.000028	0.305696
1.720271	-1.008197	0.300288	-0.000009	0.305548
1.944374	-1.081073	0.305293	-0.000051	0.305395
1.888946	-1.112593	0.310298	-0.000040	0.305198
1.662074	-1.105815	0.315302	0.000002	0.305035
1.780401	-1.158023	0.320307	-0.000020	0.304889
1.160287	-1.086362	0.325312	0.000095	0.304694
1.988721	-1.266401	0.330317	-0.000059	0.304554
1.908830	-1.299566	0.335322	-0.000044	0.304327
1.990061	-1.331506	0.340326	-0.000059	0.304245
1.690882	-1.341685	0.345331	-0.000003	0.303938
1.409400	-1.309041	0.350336	0.000049	0.303850
1.807786	-1.428256	0.355341	-0.000025	0.303627
1.639529	-1.435552	0.360346	0.000007	0.303446
1.443091	-1.428349	0.365350	0.000043	0.303310
1.334750	-1.457988	0.370355	0.000063	0.303075
1.418926	-1.496893	0.375360	0.000048	0.302962
1.508095	-1.571969	0.380365	0.000031	0.302681
1.484588	-1.604466	0.385370	0.000036	0.302505
1.314703	-1.603358	0.390374	0.000067	0.302363
1.830337	-1.761104	0.395379	-0.000029	0.302056
1.881391	-1.803329	0.400384	-0.000038	0.301898
1.931158	-1.844767	0.405389	-0.000047	0.301743
1.865194	-1.901094	0.410394	-0.000035	0.301415
1.751514	-1.915703	0.415398	-0.000014	0.301245
1.907876	-1.979560	0.420403	-0.000043	0.301075
1.743711	-2.012734	0.425408	-0.000012	0.300772
1.623998	-2.021390	0.430413	0.000010	0.300626
1.456227	-2.025151	0.435418	0.000041	0.300461
1.385649	-2.067459	0.440422	0.000054	0.300195
0.701434	-1.988408	0.445427	0.000182	0.299976
0.453902	-1.977126	0.450432	0.000228	0.299814
0.550647	-2.042106	0.455437	0.000210	0.299585
0.436494	-2.069433	0.460442	0.000231	0.299353
0.634350	-2.145375	0.465446	0.000194	0.299159
0.563406	-2.174870	0.470451	0.000208	0.298954
0.224617	-2.170736	0.475456	0.000271	0.298676
0.469391	-2.252972	0.480461	0.000225	0.298493
-0.560883	-2.097456	0.485466	0.000417	0.298339
-0.621120	-2.148968	0.490470	0.000428	0.298036
-1.158301	-2.081744	0.495475	0.000528	0.297888
-1.880409	-1.989960	0.500480	0.000663	0.297696
-1.658811	-2.079024	0.505485	0.000622	0.297459
-1.462562	-2.142974	0.510490	0.000585	0.297321
-1.348834	-2.223073	0.515494	0.000564	0.297032
-2.399587	-2.060359	0.520499	0.000760	0.296894
-2.934137	-1.986797	0.525504	0.000859	0.296779
-2.865290	-2.054762	0.530509	0.000846	0.296508
-2.827755	-2.081781	0.535514	0.000839	0.296410
-3.048511	-2.100878	0.540518	0.000880	0.296120
-3.130907	-2.108843	0.545523	0.000896	0.296008
-2.977730	-2.181633	0.550528	0.000867	0.295788
-3.004447	-2.210421	0.555533	0.000872	0.295624
-3.774688	-2.083419	0.560538	0.001016	0.295560
-3.587283	-2.189892	0.565542	0.000981	0.295205
-3.432044	-2.238012	0.570547	0.000952	0.295107
-4.288950	-2.127192	0.575552	0.001112	0.294887
-4.106349	-2.193449	0.580557	0.001078	0.294725
-4.712882	-2.113485	0.585562	0.001190	0.294576
-5.532697	-2.004951	0.590566	0.001343	0.294377
-5.547496	-2.018157	0.595571	0.001346	0.294299
-5.105085	-2.154084	0.600576	0.001264	0.294025
-5.202452	-2.152932	0.605581	0.001282	0.293944
-6.053209	-2.053537	0.610586	0.001440	0.293672
-5.660334	-2.134530	0.615590	0.001367	0.293625
-5.612284	-2.203628	0.620595	0.001358	0.293327
-6.144581	-2.117038	0.625600	0.001457	0.293277
-6.378408	-2.125645	0.630605	0.001501	0.293024
-6.393625	-2.129722	0.635610	0.001504	0.292990
-6.630304	-2.148465	0.640614	0.001548	0.292685
-6.631444	-2.160699	0.645619	0.001548	0.292623
-7.513213	-2.050065	0.650624	0.001712	0.292378
-6.739786	-2.204446	0.655629	0.001568	0.292309
-7.603303	-2.100749	0.660634	0.001729	0.292045
-7.830837	-2.062086	0.665638	0.001771	0.292032
-7.867903	-2.107628	0.670643	0.001778	0.291773
-8.603359	-1.973051	0.675648	0.001915	0.291777
-8.288327	-2.091192	0.680653	0.001857	0.291475
-8.423498	-2.075345	0.685658	0.001882	0.291432
-8.533194	-2.105413	0.690662	0.001902	0.291183
-8.856850	-2.059341	0.695667	0.001962	0.291119
-8.946362	-2.079414	0.700672	0.001979	0.290939
-8.924843	-2.109468	0.705677	0.001975	0.290809
-9.194132	-2.079867	0.710682	0.002025	0.290712
-9.563140	-2.046190	0.715686	0.002094	0.290546
-9.484737	-2.069158	0.720691	0.002079	0.290502
-10.140063	-2.009907	0.725696	0.002201	0.290204
-9.987791	-2.035744	0.730701	0.002173	0.290213
-10.269451	-2.038257	0.735706	0.002226	0.289945
-10.256130	-2.052182	0.740710	0.002223	0.289887
-10.497172	-2.038865	0.745715	0.002268	0.289735
-11.325275	-1.920359	0.750720	0.002422	0.289575
-10.610652	-2.055694	0.755725	0.002289	0.289548
-11.167815	-2.007293	0.760730	0.002393	0.289283
-10.991010	-2.041836	0.765734	0.002360	0.289271
-11.149884	-2.055617	0.770739	0.002390	0.289057
-11.402379	-2.035591	0.775744	0.002437	0.288928
-12.030358	-1.932367	0.780749	0.002554	0.288873
-12.296835	-1.927761	0.785754	0.002603	0.288653
-12.208384	-1.945494	0.790758	0.002587	0.288645
-11.908105	-2.045719	0.795763	0.002531	0.288416
-12.616487	-1.936760	0.800768	0.002663	0.288316
-12.289458	-2.007533	0.805773	0.002602	0.288259
-12.381198	-2.038730	0.810778	0.002619	0.288019
-12.618359	-1.994734	0.815782	0.002663	0.288023
-12.806735	-2.008082	0.820787	0.002698	0.287784
-13.092169	-1.976351	0.825792	0.002751	0.287682
-13.058250	-1.995842	0.830797	0.002745	0.287615
-13.381810	-1.984585	0.835802	0.002805	0.287375
-12.989089	-2.059060	0.840806	0.002732	0.287360
-13.438178	-2.021808	0.845811	0.002816	0.287136
-14.170994	-1.905934	0.850816	0.002952	0.287049
-13.369841	-2.062877	0.855821	0.002803	0.286992
-13.755714	-2.040214	0.860826	0.002875	0.286752
-14.109070	-1.975985	0.865830	0.002941	0.286752
-13.052762	-2.217990	0.870835	0.002744	0.286499
-13.940697	-2.076261	0.875840	0.002910	0.286400
-13.942795	-2.099380	0.880845	0.002910	0.286281
-15.033637	-1.933152	0.885850	0.003113	0.286119
-14.471840	-2.035450	0.890854	0.003009	0.286118
-14.716086	-2.042480	0.895859	0.003054	0.285857
-15.446962	-1.917607	0.900864	0.003190	0.285817
-14.931097	-2.025659	0.905869	0.003094	0.285744
-15.347890	-1.988303	0.910874	0.003172	0.285550
-15.745000	-1.915678	0.915878	0.003246	0.285552
-15.258822	-2.044878	0.920883	0.003155	0.285345
-15.778863	-1.977431	0.925888	0.003252	0.285207
-15.968284	-1.940959	0.930893	0.003287	0.285217
-16.063047	-1.987669	0.935898	0.003305	0.284893
-16.009648	-1.998145	0.940902	0.003295	0.284889
-16.169196	-1.991988	0.945907	0.003325	0.284772
-16.671973	-1.942820	0.950912	0.003418	0.284557
-15.873382	-2.088150	0.955917	0.003270	0.284557
-16.095066	-2.094886	0.960922	0.003311	0.284317
-16.894005	-1.957228	0.965926	0.003460	0.284278
-16.954596	-1.959826	0.970931	0.003471	0.284209
-17.463894	-1.917215	0.975936	0.003566	0.283954
-17.344212	-1.939422	0.980941	0.003544	0.283952
-17.678182	-1.905076	0.985946	0.003606	0.283817
-17.563123	-1.962922	0.990950	0.003584	0.283629
-17.533487	-1.965683	0.995955	0.003579	0.283642
-18.081065	-1.912500	1.000960	0.003681	0.283405
-18.222010	-1.900946	1.005965	0.003707	0.283333
-18.168192	-1.913384	1.010970	0.003697	0.283320
-18.364682	-1.932544	1.015974	0.003734	0.283039
-18.279892	-1.950275	1.020979	0.003718	0.283027
-18.739051	-1.872624	1.025984	0.003803	0.282997
-18.896836	-1.902053	1.030989	0.003833	0.282700
-18.975959	-1.890845	1.035994	0.003848	0.282683
-18.850345	-1.931121	1.040998	0.003824	0.282594
-18.984104	-1.949898	1.046003	0.003849	0.282373
-18.986328	-1.951803	1.051008	0.003850	0.282361
-18.342491	-2.108352	1.056013	0.003730	0.282159
-19.059236	-2.001574	1.061018	0.003863	0.282038
-19.553016	-1.910762	1.066022	0.003955	0.282043
-19.479819	-1.980776	1.071027	0.003942	0.281752
-19.726644	-1.935988	1.076032	0.003988	0.281751
-20.057083	-1.890343	1.081037	0.004049	0.281677
-20.433325	-1.868568	1.086042	0.004119	0.281437
-20.353930	-1.883129	1.091046	0.004104	0.281436
-20.262550	-1.923531	1.096051	0.004087	0.281314
-21.273952	-1.776370	1.101056	0.004276	0.281125
-20.528914	-1.911216	1.106061	0.004137	0.281128
-20.322530	-1.981627	1.111066	0.004099	0.280958
-20.861183	-1.916641	1.116070	0.004199	0.280788
-20.394760	-2.000424	1.121075	0.004112	0.280794
-20.378625	-2.045467	1.126080	0.004109	0.280576
-20.609178	-2.006801	1.131085	0.004152	0.280559
-21.139697	-1.930481	1.136090	0.004251	0.280455
-21.269138	-1.953679	1.141094	0.004275	0.280214
-20.580163	-2.079650	1.146099	0.004147	0.280210
-21.365206	-1.986292	1.151104	0.004293	0.279955
-21.762953	-1.922673	1.156109	0.004367	0.279910
-21.636743	-1.951634	1.161114	0.004343	0.279879
-22.072954	-1.931353	1.166118	0.004425	0.279573
-22.267549	-1.893338	1.171123	0.004461	0.279587
-22.394441	-1.888553	1.176128	0.004485	0.279492
-22.180968	-1.967143	1.181133	0.004445	0.279286
-22.914141	-1.829846	1.186138	0.004581	0.279306
-22.555507	-1.931698	1.191142	0.004515	0.279116
-22.524935	-1.967778	1.196147	0.004509	0.278958
-23.168704	-1.851990	1.201152	0.004629	0.278951
-23.401357	-1.853202	1.206157	0.004672	0.278725
-23.227827	-1.899149	1.211162	0.004640	0.278650
-22.881847	-1.965257	1.216166	0.004576	0.278634
-22.889653	-2.024680	1.221171	0.004577	0.278317
-23.179866	-1.973017	1.226176	0.004631	0.278311
-23.371189	-1.960215	1.231181	0.004667	0.278197
-23.936818	-1.890129	1.236186	0.004772	0.278026
-23.523120	-1.967855	1.241190	0.004695	0.278013
-23.506363	-2.018525	1.246195	0.004692	0.277765
-24.221949	-1.904174	1.251200	0.004825	0.277683
-23.630092	-2.024188	1.256205	0.004715	0.277618
-23.904800	-2.021992	1.261210	0.004766	0.277369
-24.439002	-1.922621	1.266214	0.004866	0.277380
-24.769435	-1.895720	1.271219	0.004927	0.277207
-25.071846	-1.871198	1.276224	0.004983	0.277048
-23.887990	-2.087518	1.281229	0.004763	0.277042
-24.916999	-1.948781	1.286234	0.004955	0.276789
-24.902574	-1.960169	1.291238	0.004952	0.276743
-24.250749	-2.097243	1.296243	0.004831	0.276646
-25.321945	-1.945290	1.301248	0.005030	0.276422
-25.788210	-1.854658	1.306253	0.005117	0.276452
-25.446489	-1.955724	1.311258	0.005053	0.276248
-25.487812	-1.975142	1.316262	0.005061	0.276107
-25.793669	-1.914910	1.321267	0.005118	0.276131
-26.168305	-1.905007	1.326272	0.005188	0.275825
-26.380620	-1.865634	1.331277	0.005227	0.275829
-26.780142	-1.796577	1.336282	0.005302	0.275810
-26.792775	-1.839126	1.341286	0.005304	0.275575
-26.275559	-1.930627	1.346291	0.005208	0.275588
-26.586478	-1.897037	1.351296	0.005266	0.275468
-27.058727	-1.853840	1.356301	0.005354	0.275243
-26.793885	-1.902629	1.361306	0.005304	0.275240
-26.945338	-1.909257	1.366310	0.005333	0.275060
-27.191525	-1.891091	1.371315	0.005378	0.274920
-26.976504	-1.932894	1.376320	0.005338	0.274905
-26.936324	-1.989634	1.381325	0.005331	0.274645
-27.285464	-1.938135	1.386330	0.005396	0.274581
-27.138304	-1.981594	1.391334	0.005369	0.274493
-27.147453	-2.020163	1.396339	0.005370	0.274281
-27.415732	-1.972208	1.401344	0.005420	0.274276
-27.623720	-1.980985	1.406349	0.005459	0.274030
-28.062450	-1.914733	1.411354	0.005541	0.273959
-27.380783	-2.056039	1.416358	0.005414	0.273867
-27.505380	-2.080491	1.421363	0.005437	0.273618
-27.982227	-1.994050	1.426368	0.005526	0.273616
-27.952181	-2.044794	1.431373	0.005520	0.273376
-28.260316	-2.001802	1.436378	0.005578	0.273307
-28.995474	-1.875624	1.441382	0.005715	0.273267
-28.539928	-2.002916	1.446387	0.005630	0.273031
-28.284775	-2.053156	1.451392	0.005582	0.273011
-28.788255	-2.005479	1.456397	0.005676	0.272778
-28.964002	-1.992690	1.461402	0.005709	0.272676
-29.028389	-1.990621	1.466406	0.005721	0.272625
-29.309196	-1.986245	1.471411	0.005773	0.272377
-29.484059	-1.956677	1.476416	0.005806	0.272365
-29.318546	-2.023011	1.481421	0.005775	0.272172
-30.202669	-1.881413	1.486426	0.005939	0.272070
-30.135500	-1.896436	1.491430	0.005927	0.272055
-29.576818	-2.049956	1.496435	0.005823	0.271778
-30.392371	-1.905428	1.501440	0.005975	0.271758
-30.303304	-1.939985	1.506445	0.005958	0.271660
-30.779952	-1.895492	1.511450	0.006047	0.271435
-30.458625	-1.953982	1.516454	0.005987	0.271435
-30.441245	-1.993854	1.521459	0.005984	0.271239
-31.159046	-1.884525	1.526464	0.006118	0.271125
-30.020815	-2.100558	1.531469	0.005906	0.271077
-30.583708	-2.050455	1.536474	0.006011	0.270798
-31.262147	-1.926198	1.541478	0.006137	0.270802
-30.857673	-2.025748	1.546483	0.006062	0.270663
-31.423042	-1.943801	1.551488	0.006167	0.270551
-31.811126	-1.869815	1.556493	0.006239	0.270569
-31.997468	-1.897253	1.561498	0.006274	0.270241
-32.023041	-1.897301	1.566502	0.006279	0.270216
-31.689540	-1.972042	1.571507	0.006217	0.270140
-32.297235	-1.908198	1.576512	0.006330	0.269890
-32.053098	-1.950756	1.581517	0.006284	0.269899
-32.105270	-1.978714	1.586522	0.006294	0.269698
-32.679176	-1.899746	1.591526	0.006401	0.269562
-32.147440	-1.994891	1.596531	0.006302	0.269570
-32.375010	-2.009708	1.601536	0.006344	0.269268
-32.749096	-1.937603	1.606541	0.006414	0.269290
-33.085039	-1.902867	1.611546	0.006477	0.269148
-33.427553	-1.874804	1.616550	0.006540	0.268964
-33.143383	-1.927438	1.621555	0.006488	0.268958
-33.659166	-1.875138	1.626560	0.006584	0.268735
-34.328682	-1.764652	1.631565	0.006708	0.268674
-33.885781	-1.847538	1.636570	0.006626	0.268661
-34.024232	-1.871279	1.641574	0.006652	0.268397
-34.015139	-1.886066	1.646579	0.006650	0.268326
-34.242153	-1.846325	1.651584	0.006692	0.268318
-34.225181	-1.900468	1.656589	0.006689	0.268042
-34.586169	-1.835707	1.661594	0.006756	0.268037
-34.284856	-1.907880	1.666598	0.006700	0.267943
-34.575520	-1.897690	1.671603	0.006754	0.267712
-34.867650	-1.848683	1.676608	0.006809	0.267690
-35.177389	-1.820936	1.681613	0.006866	0.267535
-34.821252	-1.914730	1.686618	0.006800	0.267378
-35.109198	-1.861590	1.691622	0.006854	0.267382
-34.496822	-2.024339	1.696627	0.006740	0.267104
-34.652203	-2.010920	1.701632	0.006769	0.267023
-34.487729	-2.062799	1.706637	0.006738	0.266904
-35.198810	-1.961287	1.711642	0.006871	0.266753
-35.521885	-1.901345	1.716646	0.006931	0.266759
-35.480716	-1.962022	1.721651	0.006923	0.266470
-35.631232	-1.944225	1.726656	0.006951	0.266418
-35.670274	-1.956707	1.731661	0.006958	0.266311
-35.701560	-1.984272	1.736666	0.006964	0.266130
-35.940902	-1.944002	1.741670	0.007009	0.266112
-36.102348	-1.962490	1.746675	0.007039	0.265852
-36.175600	-1.959533	1.751680	0.007053	0.265795
-36.228953	-1.964272	1.756685	0.007063	0.265716
-36.789604	-1.894151	1.761690	0.007167	0.265543
-37.296402	-1.798540	1.766694	0.007261	0.265561
-36.827296	-1.919136	1.771699	0.007174	0.265369
-37.777343	-1.775171	1.776704	0.007351	0.265211
-37.437619	-1.835121	1.781709	0.007288	0.265221
-37.081153	-1.948176	1.786714	0.007221	0.264958
-37.475489	-1.889748	1.791718	0.007295	0.264885
-37.242223	-1.945824	1.796723	0.007251	0.264810
-37.234266	-1.997371	1.801728	0.007250	0.264536
-37.229066	-1.996465	1.806733	0.007249	0.264546
-37.967322	-1.902160	1.811738	0.007386	0.264327
-38.058281	-1.896328	1.816742	0.007403	0.264268
-37.275946	-2.056603	1.821747	0.007258	0.264170
-38.061012	-1.960222	1.826752	0.007404	0.263915
-38.271269	-1.917571	1.831757	0.007443	0.263939
-38.065201	-2.000659	1.836762	0.007405	0.263689
-38.720466	-1.893659	1.841766	0.007527	0.263622
-38.794502	-1.891150	1.846771	0.007540	0.263561
-38.771571	-1.944920	1.851776	0.007536	0.263288
-38.659803	-1.960780	1.856781	0.007515	0.263313
-38.885229	-1.957383	1.861786	0.007557	0.263106
-39.354383	-1.890961	1.866790	0.007645	0.263002
-39.422845	-1.879097	1.871795	0.007658	0.262998
-39.752849	-1.877584	1.876800	0.007719	0.262676
-39.691727	-1.888332	1.881805	0.007708	0.262678
-39.943840	-1.863249	1.886810	0.007755	0.262563
-40.038612	-1.881433	1.891814	0.007772	0.262368
-39.890777	-1.906214	1.896819	0.007745	0.262379
-40.395732	-1.861870	1.901824	0.007839	0.262117
-40.374929	-1.878297	1.906829	0.007835	0.262047
-40.420750	-1.877542	1.911834	0.007843	0.262005
-40.977805	-1.820721	1.916838	0.007947	0.261758
-40.536145	-1.899286	1.921843	0.007865	0.261768
-40.877086	-1.864156	1.926848	0.007928	0.261619
-41.405438	-1.800452	1.931853	0.008027	0.261440
-41.031112	-1.870145	1.936858	0.007957	0.261431
-41.154111	-1.888822	1.941862	0.007980	0.261203
-41.548505	-1.830602	1.946867	0.008054	0.261128
-41.750433	-1.795948	1.951872	0.008091	0.261116
-41.169908	-1.957702	1.956877	0.007983	0.260805
-41.315915	-1.933384	1.961882	0.008010	0.260792
-41.252324	-1.972383	1.966886	0.007999	0.260640
-41.670390	-1.910957	1.971891	0.008076	0.260558
-41.951766	-1.861715	1.976896	0.008129	0.260547
-42.380314	-1.841616	1.981901	0.008209	0.260225
-42.243588	-1.867911	1.986906	0.008183	0.260217
-42.185033	-1.903204	1.991910	0.008172	0.260080
-42.971062	-1.788242	1.996915	0.008319	0.259924
-42.587817	-1.880700	2.001920	0.008247	0.259797

-42.447738	-1.950725	2.011917	0.008221	0.259549
-42.250993	-2.035257	2.021914	0.008185	0.259276
-42.522636	-2.019279	2.031910	0.008235	0.259089
-42.990199	-1.961972	2.041907	0.008322	0.258934
-43.216557	-1.961399	2.051904	0.008365	0.258706
-43.164725	-1.987391	2.061901	0.008355	0.258613
-43.695328	-1.917419	2.071898	0.008454	0.258464
-43.777041	-1.931004	2.081894	0.008469	0.258305
-43.732038	-1.939511	2.091891	0.008461	0.258303
-43.990601	-1.892578	2.101888	0.008509	0.258302
-43.937099	-1.953518	2.111885	0.008499	0.258015
-43.937639	-1.953576	2.121882	0.008499	0.258014
-43.986960	-1.944996	2.131878	0.008508	0.258011
-43.987568	-1.944067	2.141875	0.008508	0.258016
-43.333453	-2.067372	2.151872	0.008387	0.257991
-43.673324	-2.004734	2.161869	0.008450	0.257996
-43.952836	-1.949712	2.171866	0.008502	0.258019
-44.333420	-1.877284	2.181862	0.008573	0.258037
-44.168869	-1.907397	2.191859	0.008542	0.258035
-44.130889	-1.918128	2.201856	0.008535	0.258014
-44.143167	-1.914342	2.211853	0.008538	0.258022
-44.156364	-1.912344	2.221850	0.008540	0.258020
-44.312439	-1.865460	2.231846	0.008569	0.258123
-44.002643	-1.885798	2.241843	0.008512	0.258325
-44.052799	-1.878680	2.251840	0.008521	0.258314
-44.156476	-1.857827	2.261837	0.008540	0.258325
-43.479882	-1.943211	2.271834	0.008414	0.258536
-44.075146	-1.813264	2.281830	0.008525	0.258657
-44.199408	-1.788982	2.291827	0.008548	0.258666
-43.877715	-1.798290	2.301824	0.008488	0.258942
-43.574636	-1.850336	2.311821	0.008432	0.258959
-43.282350	-1.876088	2.321818	0.008378	0.259112
-42.980594	-1.900353	2.331814	0.008322	0.259283
-42.752061	-1.942187	2.341811	0.008279	0.259281
-42.975489	-1.851571	2.351808	0.008321	0.259560
-42.306097	-1.973878	2.361805	0.008196	0.259557
-42.382383	-1.917026	2.371802	0.008210	0.259796
-42.661390	-1.845071	2.381798	0.008262	0.259914
-42.375399	-1.859954	2.391795	0.008209	0.260121
-42.737774	-1.772088	2.401792	0.008276	0.260243
-41.855703	-1.882586	2.411789	0.008112	0.260521
-42.066147	-1.834482	2.421786	0.008151	0.260575
-41.515598	-1.893345	2.431782	0.008049	0.260804
-41.753153	-1.834199	2.441779	0.008093	0.260893
-41.218907	-1.891232	2.451776	0.007994	0.261115
-40.873458	-1.931551	2.461773	0.007930	0.261240
-40.778348	-1.916849	2.471770	0.007912	0.261417
-40.751200	-1.879154	2.481766	0.007907	0.261653
-40.653094	-1.873738	2.491763	0.007889	0.261782
-40.217239	-1.906027	2.501760	0.007808	0.262041
-40.259647	-1.875124	2.511757	0.007815	0.262169
-40.465111	-1.798191	2.521754	0.007854	0.262388
-39.760266	-1.877473	2.531750	0.007723	0.262657
-39.766125	-1.849077	2.541747	0.007724	0.262808
-39.664626	-1.823820	2.551744	0.007705	0.263049
-39.414231	-1.825736	2.561741	0.007658	0.263289
-39.359177	-1.805746	2.571738	0.007648	0.263453
-39.191095	-1.796989	2.581734	0.007617	0.263669
-39.124823	-1.753605	2.591731	0.007604	0.263973
-38.711494	-1.789584	2.601728	0.007527	0.264188
-38.286936	-1.835631	2.611725	0.007448	0.264359
-37.785078	-1.887449	2.621722	0.007355	0.264575
-37.485773	-1.895219	2.631718	0.007299	0.264830
-37.775879	-1.809221	2.641715	0.007353	0.265012
-37.535932	-1.810778	2.651712	0.007309	0.265241
-37.154248	-1.821951	2.661709	0.007238	0.265559
-37.208924	-1.782357	2.671706	0.007248	0.265720
-36.696060	-1.842133	2.681702	0.007152	0.265903
-36.891130	-1.759346	2.691699	0.007189	0.266160
-36.215328	-1.831905	2.701696	0.007063	0.266434
-36.098337	-1.814618	2.711693	0.007041	0.266643
-35.966577	-1.799386	2.721690	0.007017	0.266856
-35.458881	-1.851622	2.731686	0.006922	0.267073
-35.439950	-1.802957	2.741683	0.006919	0.267356
-35.133089	-1.820280	2.751680	0.006862	0.267564
-34.962736	-1.812415	2.761677	0.006830	0.267774
-34.600916	-1.827212	2.771674	0.006763	0.268049
-34.057078	-1.883356	2.781670	0.006661	0.268280
-34.045246	-1.848661	2.791667	0.006659	0.268479
-33.856163	-1.844681	2.801664	0.006624	0.268685
-33.797690	-1.802749	2.811661	0.006613	0.268968
-33.259276	-1.851455	2.821658	0.006513	0.269233
-33.317230	-1.802762	2.831654	0.006524	0.269438
-33.094108	-1.803237	2.841651	0.006482	0.269653
-32.344812	-1.890694	2.851648	0.006343	0.269915
-32.639354	-1.790490	2.861645	0.006398	0.270165
-32.264929	-1.814850	2.871642	0.006328	0.270399
-31.728803	-1.872955	2.881638	0.006228	0.270610
-31.791599	-1.818113	2.891635	0.006240	0.270842
-31.330967	-1.856328	2.901632	0.006154	0.271085
-31.139609	-1.853805	2.911629	0.006119	0.271285
-30.739678	-1.889949	2.921626	0.006044	0.271480
-30.526382	-1.871118	2.931622	0.006004	0.271787
-30.447994	-1.843775	2.941619	0.005990	0.272008
-30.330471	-1.822865	2.951616	0.005968	0.272233
-30.273807	-1.790568	2.961613	0.005957	0.272459
-29.876512	-1.811519	2.971610	0.005884	0.272731
-29.388409	-1.847552	2.981606	0.005793	0.273011
-29.228456	-1.836302	2.991603	0.005763	0.273225
-28.875893	-1.863031	3.001600	0.005697	0.273423
-28.696206	-1.847953	3.011597	0.005664	0.273675
-28.664808	-1.799275	3.021594	0.005658	0.273963
-28.440134	-1.793693	3.031590	0.005616	0.274208
-28.189687	-1.797505	3.041587	0.005570	0.274428
-27.676429	-1.855620	3.051584	0.005474	0.274614
-27.608524	-1.806631	3.061581	0.005462	0.274937
-27.077124	-1.859684	3.071578	0.005363	0.275166
-27.118015	-1.809117	3.081574	0.005370	0.275393
-26.774310	-1.826882	3.091571	0.005306	0.275627
-26.401108	-1.855838	3.101568	0.005237	0.275832
-26.144539	-1.854849	3.111565	0.005189	0.276081
-26.091620	-1.822405	3.121562	0.005179	0.276302
-26.166409	-1.762361	3.131558	0.005193	0.276545
-25.491782	-1.836635	3.141555	0.005068	0.276798
-25.375957	-1.806507	3.151552	0.005046	0.277065
-24.916285	-1.847594	3.161549	0.004961	0.277287
-24.572262	-1.870362	3.171546	0.004897	0.277495
-24.163494	-1.903542	3.181542	0.004821	0.277709
-23.910219	-1.889027	3.191539	0.004773	0.278025
-23.548107	-1.923284	3.201536	0.004706	0.278189
-23.474424	-1.902351	3.211533	0.004692	0.278367
-23.318348	-1.875677	3.221530	0.004663	0.278653
-22.883597	-1.909097	3.231526	0.004582	0.278890
-22.758999	-1.889704	3.241523	0.004559	0.279108
-22.630561	-1.873589	3.251520	0.004535	0.279313
-22.089102	-1.919065	3.261517	0.004435	0.279587
-21.921799	-1.907271	3.271514	0.004403	0.279805
-21.930593	-1.864584	3.281510	0.004405	0.280018
-21.395451	-1.919079	3.291507	0.004306	0.280239
-21.264798	-1.883414	3.301504	0.004281	0.280545
-20.682220	-1.961103	3.311501	0.004173	0.280691
-21.154934	-1.838973	3.321498	0.004261	0.280877
-20.406727	-1.926293	3.331494	0.004122	0.281128
-20.038046	-1.945138	3.341491	0.004053	0.281376
-20.166483	-1.880023	3.351488	0.004077	0.281590
-19.543686	-1.957284	3.361485	0.003961	0.281775
-19.253414	-1.958665	3.371482	0.003907	0.282039
-18.694649	-2.022857	3.381478	0.003803	0.282231
-18.044513	-2.116637	3.391475	0.003682	0.282356
-18.772108	-1.920052	3.401472	0.003817	0.282685
-18.587912	-1.906263	3.411469	0.003783	0.282927
-18.483337	-1.886639	3.421466	0.003764	0.283124
-17.707831	-1.989937	3.431462	0.003619	0.283317
-17.790098	-1.914503	3.441459	0.003635	0.283626
-17.528138	-1.923041	3.451456	0.003586	0.283825
-16.784247	-2.028664	3.461453	0.003448	0.283976
-16.927515	-1.944207	3.471450	0.003474	0.284273
-16.821571	-1.916566	3.481446	0.003454	0.284512
-16.679519	-1.899956	3.491443	0.003428	0.284727
-16.574467	-1.874286	3.501440	0.003408	0.284955
-15.860507	-1.953590	3.511437	0.003276	0.285211
-15.261543	-2.011764	3.521434	0.003164	0.285468
-15.369641	-1.960692	3.531430	0.003184	0.285627
-15.309363	-1.934143	3.541427	0.003173	0.285817
-15.078153	-1.916689	3.551424	0.003130	0.286118
-14.745363	-1.937501	3.561421	0.003068	0.286318
-14.784382	-1.891454	3.571418	0.003075	0.286515
-13.903629	-2.002273	3.581414	0.002912	0.286764
-13.691557	-1.992570	3.591411	0.002872	0.287007
-13.550450	-1.982463	3.601408	0.002846	0.287187
-13.034157	-2.041309	3.611405	0.002750	0.287364
-13.095522	-1.968145	3.621402	0.002761	0.287676
-13.118573	-1.920087	3.631398	0.002765	0.287896
-12.938752	-1.906736	3.641395	0.002732	0.288127
-12.274984	-1.987721	3.651392	0.002608	0.288326
-12.279462	-1.929674	3.661389	0.002609	0.288613
-12.133941	-1.915972	3.671386	0.002582	0.288814
-11.587746	-1.975990	3.681382	0.002481	0.289011
-11.916865	-1.855330	3.691379	0.002542	0.289315
-11.405792	-1.899887	3.701376	0.002447	0.289557
-11.150039	-1.901132	3.711373	0.002399	0.289783
-11.102968	-1.868069	3.721370	0.002390	0.289990
-10.496021	-1.928709	3.731366	0.002277	0.290238
-10.244771	-1.911559	3.741363	0.002231	0.290551
-9.947964	-1.932708	3.751360	0.002175	0.290714
-9.797939	-1.925196	3.761357	0.002148	0.290887
-9.215090	-1.980901	3.771354	0.002039	0.291137
-8.936340	-1.983238	3.781350	0.001987	0.291377
-9.087511	-1.915448	3.791347	0.002015	0.291577
-8.134389	-2.049880	3.801344	0.001838	0.291769
-8.024315	-2.017275	3.811341	0.001818	0.292030
-7.873304	-2.013021	3.821338	0.001789	0.292187
-7.080968	-2.119121	3.831334	0.001642	0.292375
-6.877735	-2.101256	3.841331	0.001604	0.292646
-6.812192	-2.084683	3.851328	0.001592	0.292786
-5.880023	-2.209727	3.861325	0.001419	0.293005
-5.466432	-2.254009	3.871322	0.001342	0.293158
-6.031176	-2.119303	3.881318	0.001447	0.293316
-6.412745	-1.990514	3.891315	0.001518	0.293609
-5.215209	-2.175139	3.901312	0.001295	0.293771
-5.145750	-2.156934	3.911309	0.001282	0.293923
-5.098958	-2.106280	3.921306	0.001273	0.294214
-4.898886	-2.110946	3.931302	0.001236	0.294370
-4.584904	-2.128051	3.941299	0.001178	0.294566
-4.947835	-2.012464	3.951296	0.001245	0.294810
-4.805301	-1.989519	3.961293	0.001219	0.295049
-4.033584	-2.096054	3.971290	0.001075	0.295214
-4.024981	-2.027927	3.981286	0.001073	0.295556
-3.993303	-2.000374	3.991283	0.001068	0.295718
-4.125596	-1.935553	4.001280	0.001092	0.295918
-5.184723	-1.682555	4.011277	0.001289	0.296213
-4.173401	-1.813567	4.021274	0.001101	0.296471
-3.902352	-1.798393	4.031270	0.001051	0.296785
-2.881286	-1.934736	4.041267	0.000861	0.297025
-2.592183	-1.941499	4.051264	0.000807	0.297248
-2.795040	-1.861397	4.061261	0.000845	0.297458
-3.076209	-1.751645	4.071258	0.000897	0.297743
-4.375093	-1.441285	4.081254	0.001139	0.298104
-3.403049	-1.557483	4.091251	0.000958	0.298397
-2.768713	-1.612442	4.101248	0.000840	0.298689
-2.102694	-1.675022	4.111245	0.000716	0.298972
-1.904831	-1.641626	4.121242	0.000679	0.299307
-2.424968	-1.491782	4.131238	0.000776	0.299574
-3.081144	-1.308228	4.141235	0.000898	0.299885
-3.265796	-1.191709	4.151232	0.000932	0.300285
-2.363331	-1.280127	4.161229	0.000764	0.300648
-1.608662	-1.365311	4.171226	0.000624	0.300898
-1.200418	-1.376998	4.181222	0.000548	0.301198
-1.374132	-1.274551	4.191219	0.000580	0.301539
-1.185224	-1.242988	4.201216	0.000545	0.301854
-1.640063	-1.094126	4.211213	0.000630	0.302172
-1.659471	-1.009577	4.221210	0.000633	0.302559
-0.541124	-1.139180	4.231206	0.000425	0.302911
-0.715566	-1.033782	4.241203	0.000457	0.303263
-0.066662	-1.082068	4.251200	0.000337	0.303594
-0.811504	-0.868518	4.261197	0.000475	0.303967
-0.211004	-0.900908	4.271194	0.000363	0.304332
-0.523583	-0.766402	4.281190	0.000422	0.304701
-0.534913	-0.678683	4.291187	0.000424	0.305107
-0.124179	-0.666469	4.301184	0.000347	0.305518
0.329929	-0.673898	4.311181	0.000263	0.305874
0.498204	-0.628917	4.321178	0.000231	0.306231
0.080204	-0.468699	4.331174	0.000309	0.306628
-0.548780	-0.257438	4.341171	0.000426	0.307085
0.141609	-0.289436	4.351168	0.000298	0.307525
0.446455	-0.255854	4.361165	0.000241	0.307943
0.186361	-0.107154	4.371162	0.000289	0.308420
0.349953	-0.048619	4.381158	0.000259	0.308833
0.096431	0.106685	4.391155	0.000306	0.309344
0.000000	0.213525	4.401152	0.000324	0.309762

-0.079793	0.504029	4.406157	0.000339	0.311048
0.019572	1.037901	4.411162	0.000320	0.313605
0.534725	1.786454	4.416166	0.000223	0.317466
0.186501	2.983889	4.421171	0.000287	0.322594
0.530152	4.337228	4.426176	0.000223	0.328882
1.174537	5.934964	4.431181	0.000102	0.336341
1.364810	7.913298	4.436186	0.000065	0.344891
1.930281	10.140953	4.441190	-0.000042	0.354532
2.300523	12.701425	4.446195	-0.000112	0.365097
2.726954	15.576268	4.451200	-0.000194	0.376614
3.485971	18.721140	4.456205	-0.000337	0.389019
4.235418	22.193803	4.461210	-0.000479	0.402215
5.231670	25.979866	4.466214	-0.000667	0.416237
5.707539	30.210892	4.471219	-0.000758	0.430981
6.767542	34.669489	4.476224	-0.000958	0.446317
8.079644	39.448436	4.481229	-0.001206	0.462290
9.051124	44.638167	4.486234	-0.001390	0.478784
10.248149	50.145331	4.491238	-0.001617	0.495774
11.159064	56.061543	4.496243	-0.001790	0.513208
12.220470	62.265509	4.501248	-0.001992	0.530926
13.244579	68.811284	4.506253	-0.002187	0.548955
14.469657	75.629845	4.511258	-0.002419	0.567198
15.538243	82.804609	4.516262	-0.002623	0.585682
17.275618	90.124035	4.521267	-0.002951	0.604233
17.908160	97.936778	4.526272	-0.003074	0.622915
19.418004	105.837771	4.531277	-0.003360	0.641606
21.283062	113.920979	4.536282	-0.003713	0.660305
22.814183	122.294368	4.541286	-0.004003	0.678978
24.095300	130.896055	4.546291	-0.004247	0.697531
25.105622	139.739694	4.551296	-0.004441	0.715993
27.122164	148.564456	4.556301	-0.004822	0.734305
28.158593	157.718668	4.561306	-0.005021	0.752468
29.758406	166.876188	4.566310	-0.005325	0.770396
31.388943	176.144173	4.571315	-0.005635	0.788128
33.015927	185.500663	4.576320	-0.005944	0.805626
34.342251	195.001934	4.581325	-0.006197	0.822911
35.522914	204.579408	4.586330	-0.006423	0.839926
37.654746	214.013026	4.591334	-0.006826	0.856643
40.070284	223.443537	4.596339	-0.007282	0.873116
40.576834	233.233416	4.601344	-0.007383	0.889320
42.251922	242.824674	4.606349	-0.007701	0.905244
43.072232	252.535439	4.611354	-0.007860	0.920844
44.519255	262.127464	4.616358	-0.008136	0.936169
46.548617	271.599100	4.621363	-0.008520	0.951218
49.430691	280.897555	4.626368	-0.009062	0.965996
53.596675	290.019986	4.631373	-0.009844	0.980619
55.349617	299.549978	4.636378	-0.010177	0.995006
57.087055	309.029734	4.641382	-0.010506	1.009110
58.718780	318.469026	4.646387	-0.010816	1.022937
60.375501	327.875560	4.651392	-0.011131	1.036537
65.752033	336.617487	4.656397	-0.012138	1.049934
67.722329	345.946473	4.661402	-0.012510	1.063154
69.029564	355.345729	4.666406	-0.012760	1.076152
70.411934	364.648339	4.671411	-0.013023	1.088882
72.144025	373.849714	4.676416	-0.013352	1.101411
74.021234	382.989873	4.681421	-0.013707	1.113751
74.941049	392.224462	4.686426	-0.013885	1.125865
75.656036	401.457703	4.691430	-0.014024	1.137803
76.444278	410.599886	4.696435	-0.014177	1.149517
77.979859	419.545944	4.701440	-0.014468	1.161029
78.973689	428.557977	4.706445	-0.014659	1.172393
80.144815	437.450740	4.711450	-0.014883	1.183540
81.071323	446.382238	4.716454	-0.015061	1.194578
81.607273	455.300344	4.721459	-0.015167	1.205419
82.337028	464.157850	4.726464	-0.015309	1.216130
83.146376	472.954892	4.731469	-0.015465	1.226692
83.888239	481.717621	4.736474	-0.015609	1.237110
85.313674	490.321563	4.741478	-0.015880	1.247391
86.219441	499.011168	4.746483	-0.016054	1.257584
87.103882	507.659761	4.751488	-0.016224	1.267645
88.484804	516.223375	4.756493	-0.016487	1.277624
90.696852	524.611628	4.761498	-0.016904	1.287486
91.425532	533.274864	4.766502	-0.017046	1.297300
91.997090	541.926204	4.771507	-0.017158	1.306997
92.753021	550.569250	4.776512	-0.017304	1.316648
93.629608	559.066371	4.781517	-0.017473	1.326091
94.826935	567.513037	4.786522	-0.017701	1.335470
95.750296	575.985073	4.791526	-0.017879	1.344762
96.599659	584.468407	4.796531	-0.018042	1.353988
98.014797	592.807071	4.801536	-0.018311	1.363099
99.767897	601.148514	4.806541	-0.018643	1.372210
100.679418	609.601153	4.811546	-0.018818	1.381230
102.013197	617.977309	4.816550	-0.019072	1.390185
102.980258	626.392740	4.821555	-0.019258	1.399060
103.406775	634.881283	4.826560	-0.019343	1.407861
104.227225	643.294655	4.831565	-0.019501	1.416597
104.742102	651.728902	4.836570	-0.019602	1.425250
106.450047	659.966197	4.841574	-0.019926	1.433850
107.859522	668.234998	4.846579	-0.020193	1.442380
108.963220	676.553294	4.851584	-0.020404	1.450859
109.138040	685.048193	4.856589	-0.020442	1.459311
109.668905	693.443292	4.861594	-0.020547	1.467674
110.367934	701.809163	4.866598	-0.020682	1.475988
110.687404	710.178255	4.871603	-0.020747	1.484198
112.215807	718.360703	4.876608	-0.021037	1.492373
113.556318	726.583527	4.881613	-0.021292	1.500513
114.193462	734.924566	4.886618	-0.021416	1.508611
115.622717	743.114711	4.891622	-0.021688	1.516645
116.265972	751.434985	4.896627	-0.021813	1.524638
116.352372	759.870284	4.901632	-0.021834	1.532612
116.631541	768.219166	4.906637	-0.021892	1.540493
117.906543	776.371025	4.911642	-0.022134	1.548302
119.178583	784.549484	4.916646	-0.022377	1.556094
120.008500	792.802790	4.921651	-0.022537	1.563851
120.649054	801.101418	4.926656	-0.022661	1.571582
121.022701	809.429529	4.931661	-0.022736	1.579262
121.328961	817.729036	4.936666	-0.022799	1.586870
122.075485	825.953458	4.941670	-0.022943	1.594437
123.127923	834.119387	4.946675	-0.023144	1.601960
123.588027	842.390481	4.951680	-0.023235	1.609456
124.000676	850.690682	4.956685	-0.023317	1.616937
124.812051	858.871124	4.961690	-0.023474	1.624333
125.883019	867.068366	4.966694	-0.023679	1.631747
126.756388	875.265005	4.971699	-0.023847	1.639099
127.756885	883.401466	4.976704	-0.024038	1.646383
128.516375	891.626490	4.981709	-0.024185	1.653678
129.266231	899.808469	4.986714	-0.024330	1.660902
130.469375	907.962890	4.991718	-0.024559	1.668133
131.691397	916.082876	4.996723	-0.024792	1.675305
132.433506	924.300150	5.001728	-0.024935	1.682464
132.836992	932.602426	5.006733	-0.025016	1.689620
133.365172	940.825116	5.011738	-0.025120	1.696694
134.233190	948.989860	5.016742	-0.025287	1.703735
134.456431	957.280872	5.021747	-0.025334	1.710768
135.009613	965.463831	5.026752	-0.025442	1.717725
136.019490	973.581334	5.031757	-0.025635	1.724658
136.247187	981.841679	5.036762	-0.025683	1.731580
136.536191	990.086570	5.041766	-0.025742	1.738470
137.072878	998.255322	5.046771	-0.025847	1.745302
137.803180	1006.391210	5.051776	-0.025989	1.752104
138.241128	1014.593102	5.056781	-0.026076	1.758897
139.184654	1022.674301	5.061786	-0.026256	1.765629
140.170056	1030.808224	5.066790	-0.026445	1.772384
140.637719	1039.030715	5.071795	-0.026538	1.779119
141.415115	1047.155003	5.076800	-0.026688	1.785789
142.615522	1055.267919	5.081805	-0.026916	1.792477
143.023993	1063.463369	5.086810	-0.026998	1.799107
143.340884	1071.659710	5.091814	-0.027062	1.805702
143.622056	1079.888953	5.096819	-0.027120	1.812295
143.804210	1088.085219	5.101824	-0.027159	1.818825
144.177369	1096.245839	5.106829	-0.027234	1.825327
144.688502	1104.383693	5.111834	-0.027334	1.831805
145.120846	1112.536150	5.116838	-0.027420	1.838262
145.794311	1120.623636	5.121843	-0.027551	1.844674
147.082460	1128.653175	5.126848	-0.027796	1.851092
148.393747	1136.703837	5.131853	-0.028045	1.857507
148.747564	1144.919199	5.136858	-0.028116	1.863914
149.622710	1153.045822	5.141862	-0.028285	1.870291
150.894100	1161.110705	5.146867	-0.028527	1.876645
151.099750	1169.345401	5.151872	-0.028570	1.882983
151.461718	1177.529565	5.156877	-0.028643	1.889280
152.207783	1185.626994	5.161882	-0.028787	1.895534
152.916602	1193.763305	5.166886	-0.028925	1.901792
153.207182	1201.946865	5.171891	-0.028984	1.908017
153.177587	1210.199425	5.176896	-0.028984	1.914237
154.453750	1218.165366	5.181901	-0.029227	1.920370
154.883591	1226.310729	5.186906	-0.029312	1.926522
155.447675	1234.462439	5.191910	-0.029422	1.932674
156.588385	1242.505662	5.196915	-0.029640	1.938791
156.843019	1250.674853	5.201920	-0.029693	1.944882
157.586486	1258.810836	5.206925	-0.029836	1.950984
157.821053	1266.961133	5.211930	-0.029885	1.957021
158.917047	1274.987819	5.216934	-0.030095	1.963043
159.256957	1283.168087	5.221939	-0.030163	1.969077
159.519815	1291.330534	5.226944	-0.030217	1.975070
160.607698	1299.358276	5.231949	-0.030425	1.981036
161.505009	1307.409731	5.236954	-0.030597	1.986981
161.721436	1315.630466	5.241958	-0.030643	1.992957
162.289846	1323.751502	5.246963	-0.030754	1.998881
162.540902	1331.894856	5.251968	-0.030806	2.004770
162.972478	1340.042080	5.256973	-0.030892	2.010663
163.179775	1348.187903	5.261978	-0.030936	2.016514
164.115992	1356.205455	5.266982	-0.031115	2.022333
164.759962	1364.306650	5.271987	-0.031241	2.028165
164.756270	1372.534763	5.276992	-0.031245	2.034001
165.527342	1380.575972	5.281997	-0.031394	2.039770
165.963001	1388.671889	5.287002	-0.031480	2.045525
166.063080	1396.840410	5.292006	-0.031504	2.051281
166.605020	1404.930430	5.297011	-0.031610	2.057011
167.720723	1412.928787	5.302016	-0.031823	2.062720
169.157358	1420.907846	5.307021	-0.032096	2.068432
169.952818	1429.020922	5.312026	-0.032249	2.074156
170.657105	1437.130741	5.317030	-0.032386	2.079853
171.541315	1445.209068	5.322035	-0.032556	2.085530
172.100940	1453.369723	5.327040	-0.032665	2.091215
172.679310	1461.500785	5.332045	-0.032778	2.096867
173.385695	1469.591205	5.337050	-0.032915	2.102488
174.366429	1477.651879	5.342054	-0.033103	2.108100
175.381395	1485.741540	5.347059	-0.033297	2.113721
176.358893	1493.790994	5.352064	-0.033484	2.119296
176.816996	1501.923072	5.357069	-0.033575	2.124860
177.088907	1510.088740	5.362074	-0.033631	2.130415
177.980559	1518.147623	5.367078	-0.033802	2.135943
178.306368	1526.292459	5.372083	-0.033868	2.141460
178.787775	1534.405457	5.377088	-0.033963	2.146956
179.769262	1542.456798	5.382093	-0.034151	2.152445
180.285410	1550.558116	5.387098	-0.034252	2.157908
180.921353	1558.620999	5.392102	-0.034376	2.163343
181.554815	1566.715120	5.397107	-0.034499	2.168785
181.913021	1574.863044	5.402112	-0.034571	2.174223
182.531941	1582.950263	5.407117	-0.034692	2.179632
183.147572	1591.000729	5.412122	-0.034812	2.185002
183.264084	1599.204721	5.417126	-0.034839	2.190413
183.918087	1607.257506	5.422131	-0.034966	2.195762
184.664806	1615.291499	5.427136	-0.035110	2.201094
185.742482	1623.304851	5.432141	-0.035316	2.206431
185.976787	1631.477682	5.437146	-0.035365	2.211780
186.373861	1639.598212	5.442150	-0.035444	2.217097
187.055256	1647.628066	5.447155	-0.035576	2.222368
187.925011	1655.648292	5.452160	-0.035743	2.227638
188.626399	1663.766806	5.457165	-0.035879	2.232943
188.871950	1671.877745	5.462170	-0.035930	2.238190
189.209138	1679.975102	5.467174	-0.035998	2.243423
189.604135	1688.090350	5.472179	-0.036077	2.248661
190.159305	1696.143025	5.477184	-0.036185	2.253861
190.419369	1704.295385	5.482189	-0.036239	2.259086
190.850324	1712.369080	5.487194	-0.036325	2.264264
192.067214	1720.342451	5.492198	-0.036556	2.269436
192.987143	1728.391511	5.497203	-0.036733	2.274618
193.617065	1736.441809	5.502208	-0.036855	2.279763
194.056348	1744.554055	5.507213	-0.036943	2.284919
194.621008	1752.623625	5.512218	-0.037053	2.290047
195.716958	1760.633201	5.517222	-0.037262	2.295172
196.539792	1768.683240	5.522227	-0.037421	2.300287
197.117633	1776.793092	5.527232	-0.037534	2.305406
197.744659	1784.900084	5.532237	-0.037656	2.310517
198.566625	1792.928602	5.537242	-0.037814	2.315584
198.775080	1801.080464	5.542246	-0.037858	2.320664
199.205731	1809.170181	5.547251	-0.037943	2.325713
199.455412	1817.279832	5.552256	-0.037995	2.330748
200.436108	1825.287705	5.557261	-0.038183	2.335772
200.386300	1833.454519	5.562266	-0.038179	2.340795
201.243736	1841.453801	5.567270	-0.038344	2.345780
201.806819	1849.543677	5.572275	-0.038454	2.350786
201.980280	1857.656156	5.577280	-0.038491	2.355763
202.952801	1865.653080	5.582285	-0.038678	2.360724
203.345276	1873.729227	5.587290	-0.038756	2.365676
203.793054	1881.835652	5.592294	-0.038845	2.370640
203.967399	1889.972395	5.597299	-0.038882	2.375589
204.309116	1898.029283	5.602304	-0.038951	2.380493
204.912408	1906.072160	5.607309	-0.039069	2.385400
205.070105	1914.201077	5.612314	-0.039104	2.390313
205.502424	1922.270690	5.617318	-0.039189	2.395202
206.436663	1930.235833	5.622323	-0.039368	2.400058
207.230141	1938.237653	5.627328	-0.039521	2.404915
207.871871	1946.316227	5.632333	-0.039646	2.409796
208.015827	1954.463736	5.637338	-0.039678	2.414669
208.711025	1962.509636	5.642342	-0.039813	2.419515
209.393825	1970.538551	5.647347	-0.039945	2.424339
209.335470	1978.718367	5.652352	-0.039940	2.429186
210.056522	1986.783752	5.657357	-0.040079	2.434016
210.432587	1994.806647	5.662362	-0.040154	2.438784
210.813525	2002.881698	5.667366	-0.040231	2.443574
212.059410	2010.830835	5.672371	-0.040468	2.448347
212.792156	2018.867269	5.677376	-0.040609	2.453123
213.725359	2026.892619	5.682381	-0.040788	2.457898
214.172334	2034.989130	5.687386	-0.040877	2.462668
214.697558	2043.120799	5.692390	-0.040980	2.467455
215.743907	2051.121085	5.697395	-0.041180	2.472196
216.045499	2059.223745	5.702400	-0.041241	2.476930
216.593913	2067.316542	5.707405	-0.041349	2.481668
216.970004	2075.361907	5.712410	-0.041424	2.486357
217.990266	2083.367847	5.717414	-0.041619	2.491063
218.488445	2091.471959	5.722419	-0.041717	2.495776
218.875840	2099.558657	5.727424	-0.041795	2.500463
219.316891	2107.641040	5.732429	-0.041882	2.505142
219.492133	2115.768396	5.737434	-0.041920	2.509818
220.317110	2123.760328	5.742438	-0.042079	2.514456
220.072709	2131.920846	5.747443	-0.042038	2.519103
220.437880	2139.942290	5.752448	-0.042112	2.523707
220.932831	2147.995633	5.757453	-0.042209	2.528330
221.632404	2155.992904	5.762458	-0.042345	2.532928
222.554376	2163.985933	5.767462	-0.042521	2.537531
223.167972	2172.041080	5.772467	-0.042641	2.542138
222.922218	2180.247861	5.777472	-0.042600	2.546760
223.888807	2188.217982	5.782477	-0.042786	2.551328
223.977371	2196.315695	5.787482	-0.042807	2.555896
225.255215	2204.250735	5.792486	-0.043050	2.560450
225.937127	2212.286325	5.797491	-0.043183	2.565009
226.182977	2220.423870	5.802496	-0.043234	2.569586
226.911406	2228.462594	5.807501	-0.043375	2.574134
227.305608	2236.535686	5.812506	-0.043453	2.578669
228.194322	2244.506002	5.817510	-0.043624	2.583174
228.344245	2252.670342	5.822515	-0.043657	2.587726
228.203098	2260.888973	5.827520	-0.043636	2.592281
228.626132	2268.958205	5.832525	-0.043720	2.596784
228.733241	2276.974445	5.837530	-0.043745	2.601227
229.211916	2284.969691	5.842534	-0.043840	2.605678
229.773978	2292.995647	5.847539	-0.043949	2.610143
229.787966	2301.090392	5.852544	-0.043957	2.614601
230.536494	2309.067949	5.857549	-0.044102	2.619037
230.767118	2317.109591	5.862554	-0.044150	2.623465
231.038845	2325.204627	5.867558	-0.044206	2.627918
231.705364	2333.221606	5.872563	-0.044335	2.632348
232.325044	2341.223115	5.877568	-0.044456	2.636758
233.204850	2349.238543	5.882573	-0.044625	2.641185
233.285258	2357.323556	5.887578	-0.044645	2.645590
233.839023	2365.399549	5.892582	-0.044753	2.650013
234.614988	2373.419896	5.897587	-0.044903	2.654414
235.366180	2381.429662	5.902592	-0.045048	2.658800
236.166481	2389.480604	5.907597	-0.045202	2.663205
237.005619	2397.505845	5.912602	-0.045364	2.667590
236.799069	2405.713034	5.917606	-0.045331	2.671997
237.412661	2413.709505	5.922611	-0.045450	2.676338
237.843664	2421.732330	5.927616	-0.045536	2.680673
238.174037	2429.815662	5.932621	-0.045602	2.685027
237.981997	2437.941510	5.937626	-0.045572	2.689363
238.637415	2445.956827	5.942630	-0.045699	2.693688
239.116008	2453.990489	5.947635	-0.045794	2.698004
239.863265	2461.934329	5.952640	-0.045938	2.702283
240.065679	2470.041771	5.957645	-0.045981	2.706607
240.248719	2478.138159	5.962650	-0.046020	2.710916
240.670999	2486.183311	5.967654	-0.046104	2.715207
241.043014	2494.232737	5.972659	-0.046179	2.719490
241.836839	2502.195269	5.977664	-0.046332	2.723747
242.650062	2510.229410	5.982669	-0.046488	2.728037
242.916059	2518.344639	5.987674	-0.046543	2.732327
243.332931	2526.400066	5.992678	-0.046626	2.736589
243.779105	2534.467181	5.997683	-0.046714	2.740852
244.531201	2542.435531	6.002688	-0.046859	2.745076
245.012455	2550.502574	6.007693	-0.046954	2.749328
245.565622	2558.592379	6.012698	-0.047062	2.753589
246.253608	2566.561667	6.017702	-0.047196	2.757790
246.596766	2574.644940	6.022707	-0.047265	2.762022
246.854101	2582.704712	6.027712	-0.047318	2.766230
247.223981	2590.780468	6.032717	-0.047392	2.770446
247.546020	2598.827388	6.037722	-0.047457	2.774638
247.869898	2606.879815	6.042726	-0.047523	2.778827
248.246516	2614.924488	6.047731	-0.047598	2.783009
248.799734	2622.939581	6.052736	-0.047706	2.787179
248.863779	2631.073996	6.057741	-0.047724	2.791376
249.190223	2639.112308	6.062746	-0.047790	2.795532
249.944638	2647.076953	6.067750	-0.047935	2.799670
250.606338	2655.078624	6.072755	-0.048064	2.803815
250.622061	2663.179243	6.077760	-0.048072	2.807966
251.453231	2671.205725	6.082765	-0.048232	2.812121
251.543717	2679.285770	6.087770	-0.048254	2.816254
251.784377	2687.356687	6.092774	-0.048304	2.820385
252.575355	2695.331831	6.097779	-0.048456	2.824493
253.190704	2703.357725	6.102784	-0.048576	2.828611
253.995811	2711.397814	6.107789	-0.048731	2.832740
254.609175	2719.422226	6.112794	-0.048851	2.836845
254.845026	2727.497608	6.117798	-0.048900	2.840947
255.224444	2735.550436	6.122803	-0.048976	2.845040
255.586613	2743.576207	6.127808	-0.049049	2.849113
256.419647	2751.608881	6.132813	-0.049209	2.853210
256.404583	2759.703052	6.137818	-0.049211	2.857284
257.305258	2767.661711	6.142822	-0.049384	2.861336
257.815705	2775.696391	6.147827	-0.049484	2.865398
258.551410	2783.699774	6.152832	-0.049627	2.869451
258.985909	2791.808900	6.157837	-0.049713	2.873535
259.408081	2799.832435	6.162842	-0.049797	2.877569
259.927577	2807.871518	6.167846	-0.049899	2.881610
260.248452	2815.936392	6.172851	-0.049964	2.885647
260.397386	2824.031440	6.177856	-0.049997	2.889684
260.454729	2832.164519	6.182861	-0.050013	2.893730
260.616033	2840.221204	6.187866	-0.050048	2.897737
261.272147	2848.179607	6.192870	-0.050175	2.901718
261.886648	2856.186140	6.197875	-0.050295	2.905714
261.563870	2864.329317	6.202880	-0.050240	2.909721
261.708997	2872.456835	6.207885	-0.050272	2.913740
262.246538	2880.407576	6.212890	-0.050378	2.917688
262.634097	2888.402507	6.217894	-0.050455	2.921644
262.785336	2896.437812	6.222899	-0.050488	2.925602
263.339600	2904.409032	6.227904	-0.050597	2.929545
264.257864	2912.409807	6.232909	-0.050773	2.933516
264.381995	2920.472934	6.237914	-0.050801	2.937470
264.302744	2928.597458	6.242918	-0.050792	2.941438
264.851055	2936.614833	6.247923	-0.050899	2.945381
265.135114	2944.636934	6.252928	-0.050957	2.949307
265.709491	2952.685008	6.257933	-0.051069	2.953256
265.895648	2960.721614	6.262938	-0.051109	2.957174
265.718185	2968.836875	6.267942	-0.051081	2.961105
266.238522	2976.815499	6.272947	-0.051183	2.965002
266.599930	2984.826658	6.277952	-0.051256	2.968900
267.473648	2992.792433	6.282957	-0.051424	2.972799
267.525919	3000.922595	6.287962	-0.051439	2.976728
268.092870	3008.914105	6.292966	-0.051550	2.980613
268.631823	3016.955680	6.297971	-0.051655	2.984515
268.532690	3025.049386	6.302976	-0.051642	2.988403
268.848284	3033.125998	6.307981	-0.051706	2.992300
269.568585	3041.076873	6.312986	-0.051845	2.996153
270.040380	3049.076667	6.317990	-0.051938	3.000010
270.539093	3057.103072	6.322995	-0.052036	3.003877
270.386755	3065.225773	6.328000	-0.052013	3.007752
270.410758	3073.325730	6.333005	-0.052023	3.011620
270.478558	3081.382983	6.338010	-0.052041	3.015465
270.538532	3089.392999	6.343014	-0.052057	3.019282
271.651160	3097.267076	6.348019	-0.052270	3.023082
271.670653	3105.368309	6.353024	-0.052278	3.026930
272.233590	3113.406161	6.358029	-0.052388	3.030771
273.052678	3121.358997	6.363034	-0.052546	3.034579
273.668087	3129.397779	6.368038	-0.052666	3.038413
273.789542	3137.499444	6.373043	-0.052694	3.042247
274.317311	3145.525232	6.378048	-0.052797	3.046061
274.592914	3153.628106	6.383053	-0.052854	3.049893
275.323857	3161.569796	6.388058	-0.052995	3.053668
275.612001	3169.644811	6.393062	-0.053054	3.057478
275.860969	3177.737448	6.398067	-0.053106	3.061290
276.088012	3185.739328	6.403072	-0.053153	3.065054
276.447919	3193.820138	6.408077	-0.053225	3.068856
276.450458	3201.930004	6.413082	-0.053231	3.072650
277.226851	3209.887972	6.418086	-0.053381	3.076405
276.792884	3218.032023	6.423091	-0.053305	3.080185
276.675821	3226.031362	6.428096	-0.053289	3.083907
277.540717	3234.010229	6.433101	-0.053455	3.087663
278.393339	3241.955501	6.438106	-0.053619	3.091397
278.659917	3250.017022	6.443110	-0.053674	3.095153
278.490299	3258.128846	6.448115	-0.053647	3.098908
278.726778	3266.122171	6.453120	-0.053697	3.102622
279.085852	3274.164081	6.458125	-0.053769	3.106359
279.493413	3282.215017	6.463130	-0.053850	3.110099
280.220955	3290.177883	6.468134	-0.053991	3.113808
281.058632	3298.149006	6.473139	-0.054152	3.117522
280.663047	3306.307770	6.478144	-0.054083	3.121260
281.642280	3314.209660	6.483149	-0.054271	3.124939
281.791108	3322.305258	6.488154	-0.054304	3.128665
282.176922	3330.364411	6.493158	-0.054381	3.132380
282.410818	3338.444414	6.498163	-0.054430	3.136093
282.691595	3346.461198	6.503168	-0.054487	3.139775
283.088322	3354.478743	6.508173	-0.054566	3.143459
283.533126	3362.480606	6.513178	-0.054654	3.147133
283.814307	3370.539082	6.518182	-0.054712	3.150821
284.473165	3378.544438	6.523187	-0.054840	3.154497
284.498353	3386.597969	6.528192	-0.054850	3.158163
285.014112	3394.627003	6.533197	-0.054951	3.161835
285.536193	3402.608589	6.538202	-0.055053	3.165481
285.328742	3410.721496	6.543206	-0.055020	3.169151
286.207576	3418.692541	6.548211	-0.055189	3.172800
286.711789	3426.719479	6.553216	-0.055288	3.176453
286.865477	3434.841253	6.558221	-0.055322	3.180129
287.056492	3442.829755	6.563226	-0.055363	3.183743
287.246202	3450.914181	6.568230	-0.055403	3.187396
287.985590	3458.920724	6.573235	-0.055546	3.191033
288.017045	3466.927455	6.578240	-0.055557	3.194636
288.518069	3474.967459	6.583245	-0.055656	3.198269
289.111302	3482.934891	6.588250	-0.055771	3.201870
289.329226	3490.997151	6.593254	-0.055817	3.205493
289.577236	3499.064368	6.598259	-0.055868	3.209116
289.528631	3507.167829	6.603264	-0.055865	3.212738
290.009790	3515.209528	6.608269	-0.055959	3.216351
289.854579	3523.254678	6.613274	-0.055936	3.219934
289.945001	3531.255913	6.618278	-0.055958	3.223504
290.626287	3539.245751	6.623283	-0.056090	3.227090
290.996258	3547.280641	6.628288	-0.056164	3.230678
291.250439	3555.320838	6.633293	-0.056217	3.234261
292.186889	3563.215588	6.638298	-0.056396	3.237803
292.156298	3571.352178	6.643302	-0.056396	3.241408
292.254058	3579.360165	6.648307	-0.056419	3.244957
292.218661	3587.440319	6.653312	-0.056418	3.248529
292.598951	3595.483384	6.658317	-0.056494	3.252098
292.625279	3603.562871	6.663322	-0.056504	3.255664
293.178902	3611.500048	6.668326	-0.056612	3.259185
293.255754	3619.613161	6.673331	-0.056632	3.262761
293.714606	3627.583289	6.678336	-0.056722	3.266285
294.385279	3635.558996	6.683341	-0.056852	3.269816
294.459762	3643.622953	6.688346	-0.056871	3.273358
294.967271	3651.598753	6.693350	-0.056971	3.276875
294.948613	3659.701700	6.698355	-0.056973	3.280422
296.073438	3667.549175	6.703360	-0.057187	3.283900
296.403577	3675.654196	6.708365	-0.057254	3.287455
296.393860	3683.777762	6.713370	-0.057258	3.291000
296.772683	3691.790821	6.718374	-0.057333	3.294509
296.786249	3699.893919	6.723379	-0.057341	3.298039
296.817950	3707.927959	6.728384	-0.057352	3.301536
297.741490	3715.813513	6.733389	-0.057529	3.304999
297.552190	3723.994798	6.738394	-0.057499	3.308544
297.927379	3731.998413	6.743398	-0.057575	3.312029
298.040109	3740.063128	6.748403	-0.057601	3.315528
298.515923	3747.992637	6.753408	-0.057695	3.318978
298.540913	3756.080163	6.758413	-0.057704	3.322475
299.101805	3764.058844	6.763418	-0.057814	3.325942
299.734093	3772.028169	6.768422	-0.057937	3.329404
299.648656	3780.175864	6.773427	-0.057926	3.332912
300.036685	3788.186265	6.778432	-0.058004	3.336376
300.867171	3796.138340	6.783437	-0.058164	3.339827
300.827936	3804.207278	6.788442	-0.058162	3.343292
301.033654	3812.261491	6.793446	-0.058205	3.346756
300.917802	3820.371430	6.798451	-0.058189	3.350228
301.697770	3828.258543	6.803456	-0.058339	3.353635
302.218889	3836.320599	6.808461	-0.058441	3.357104
302.493243	3844.330985	6.813466	-0.058498	3.360537
302.353196	3852.385156	6.818470	-0.058477	3.363971
303.400498	3860.330133	6.823475	-0.058677	3.367398
303.985076	3868.367928	6.828480	-0.058791	3.370844
304.294045	3876.428599	6.833485	-0.058854	3.374286
304.385856	3884.481917	6.838490	-0.058876	3.377713
304.822182	3892.510779	6.843494	-0.058963	3.381140
305.352298	3900.509739	6.848499	-0.059067	3.384553
305.402625	3908.603959	6.853504	-0.059081	3.387985
305.656240	3916.716282	6.858509	-0.059134	3.391430
306.082949	3924.723221	6.863514	-0.059218	3.394832
306.318406	3932.701506	6.868518	-0.059267	3.398212
305.991397	3940.833424	6.873523	-0.059212	3.401633
306.574015	3948.704999	6.878528	-0.059325	3.404974
307.142087	3956.750409	6.883533	-0.059436	3.408383
307.704893	3964.773430	6.888538	-0.059546	3.411780
308.144514	3972.789114	6.893542	-0.059633	3.415166
308.819924	3980.788657	6.898547	-0.059764	3.418550
308.669319	3988.887415	6.903552	-0.059742	3.421943
309.092659	3996.906564	6.908557	-0.059826	3.425319
309.652778	4004.903752	6.913562	-0.059935	3.428688
310.152336	4012.905915	6.918566	-0.060033	3.432053
310.535725	4020.999083	6.923571	-0.060110	3.435449
311.185357	4028.908527	6.928576	-0.060236	3.438774
311.413661	4037.006853	6.933581	-0.060284	3.442160
311.208604	4045.064365	6.938586	-0.060251	3.445510
311.891970	4053.043654	6.943590	-0.060383	3.448855
311.860115	4061.197225	6.948595	-0.060383	3.452245
312.026625	4069.210969	6.953600	-0.060419	3.455581
312.656849	4077.156216	6.958605	-0.060541	3.458900
313.103892	4085.177079	6.963610	-0.060630	3.462241
313.153616	4093.248819	6.968614	-0.060644	3.465587
313.499449	4101.301314	6.973619	-0.060714	3.468931
313.320854	4109.395943	6.978624	-0.060686	3.472272
313.984526	4117.358356	6.983629	-0.060815	3.475583
314.216666	4125.311259	6.988634	-0.060863	3.478873
314.512106	4133.367474	6.993638	-0.060923	3.482204
315.158163	4141.310129	6.998643	-0.061049	3.485497
315.350282	4149.342495	7.003648	-0.061090	3.488808
315.716657	4157.431734	7.008653	-0.061163	3.492145
315.979700	4165.470197	7.013658	-0.061217	3.495455
315.934959	4173.510421	7.018662	-0.061214	3.498753
316.882276	4181.466605	7.023667	-0.061396	3.502045
316.913154	4189.526088	7.028672	-0.061407	3.505347
317.532417	4197.549060	7.033677	-0.061527	3.508649
317.760548	4205.584686	7.038682	-0.061575	3.511941
318.282041	4213.599581	7.043686	-0.061677	3.515230
318.613368	4221.634828	7.048691	-0.061744	3.518519
318.804931	4229.676409	7.053696	-0.061785	3.521803
319.391919	4237.684044	7.058701	-0.061900	3.525082
319.764791	4245.698396	7.063706	-0.061974	3.528354
320.037326	4253.771950	7.068710	-0.062030	3.531644
320.467569	4261.787127	7.073715	-0.062116	3.534913
320.719942	4269.812866	7.078720	-0.062168	3.538176
320.861717	4277.872374	7.083725	-0.062200	3.541447
321.148224	4285.868903	7.088730	-0.062258	3.544694
321.178633	4293.942691	7.093734	-0.062269	3.547961
321.909780	4301.975853	7.098739	-0.062410	3.551231
322.001424	4310.016729	7.103744	-0.062433	3.554480
322.908194	4317.910967	7.108749	-0.062607	3.557693
323.311569	4325.960166	7.113754	-0.062687	3.560949
323.937523	4333.882984	7.118758	-0.062809	3.564159
323.691128	4342.074627	7.123763	-0.062768	3.567447
324.116734	4350.097319	7.128768	-0.062853	3.570684
324.946524	4358.061413	7.133773	-0.063012	3.573908
324.668470	4366.173535	7.138778	-0.062966	3.577154
324.998270	4374.150948	7.143782	-0.063032	3.580361
325.772842	4382.097907	7.148787	-0.063182	3.583567
325.977567	4390.166439	7.153792	-0.063225	3.586801
326.143637	4398.223337	7.158797	-0.063261	3.590027
326.146739	4406.299592	7.163802	-0.063267	3.593253
326.511508	4414.271172	7.168806	-0.063340	3.596444
326.988477	4422.244904	7.173811	-0.063434	3.599637
327.001839	4430.271643	7.178816	-0.063442	3.602835
327.751216	4438.320852	7.183821	-0.063587	3.606060
327.652009	4446.390706	7.188826	-0.063573	3.609266
327.840116	4454.446831	7.193830	-0.063614	3.612471
328.417499	4462.459187	7.198835	-0.063726	3.615668
328.445149	4470.460325	7.203840	-0.063737	3.618841
329.292794	4478.420471	7.208845	-0.063900	3.622019
329.453878	4486.464942	7.213850	-0.063935	3.625208
329.830889	4494.501896	7.218854	-0.064010	3.628397
329.920847	4502.583208	7.223859	-0.064032	3.631593
330.077903	4510.580669	7.228864	-0.064067	3.634754
330.528883	4518.591999	7.233869	-0.064156	3.637927
330.924250	4526.623986	7.238874	-0.064235	3.641103
331.126324	4534.581641	7.243878	-0.064278	3.644242
331.601254	4542.636591	7.248883	-0.064371	3.647424
331.845497	4550.672098	7.253888	-0.064422	3.650589
332.141473	4558.717433	7.258893	-0.064482	3.653757
332.503575	4566.754921	7.263898	-0.064555	3.656920
332.683316	4574.783566	7.268902	-0.064594	3.660073
333.274922	4582.744347	7.273907	-0.064709	3.663207
333.840408	4590.749945	7.278912	-0.064819	3.666355
334.282017	4598.803998	7.283917	-0.064907	3.669516
334.564408	4606.838595	7.288922	-0.064965	3.672662
335.054453	4614.856347	7.293926	-0.065061	3.675805
335.254527	4622.869018	7.298931	-0.065104	3.678935
335.346895	4630.912801	7.303936	-0.065126	3.682072
335.205152	4638.987463	7.308941	-0.065105	3.685212
335.758952	4646.926157	7.313946	-0.065213	3.688314
336.139554	4654.977546	7.318950	-0.065289	3.691453
336.112626	4663.077968	7.323955	-0.065290	3.694598
336.768815	4670.992773	7.328960	-0.065417	3.697686
337.187658	4679.069010	7.333965	-0.065500	3.700828
336.850620	4687.124689	7.338970	-0.065443	3.703939
337.095949	4695.164266	7.343974	-0.065493	3.707057
337.971914	4703.124328	7.348979	-0.065662	3.710157
338.195850	4711.175946	7.353984	-0.065709	3.713274
338.542941	4719.220622	7.358989	-0.065779	3.716388
338.972270	4727.175276	7.363994	-0.065864	3.719467
339.172924	4735.209303	7.368998	-0.065906	3.722568
339.133105	4743.325110	7.374003	-0.065904	3.725692
339.793099	4751.237970	7.379008	-0.066032	3.728753
340.117085	4759.297351	7.384013	-0.066098	3.731859
340.237959	4767.362973	7.389018	-0.066125	3.734960
340.200261	4775.396800	7.394022	-0.066124	3.738042
340.589012	4783.447984	7.399027	-0.066201	3.741138
340.522638	4791.373914	7.404032	-0.066194	3.744173
341.108378	4799.416137	7.409037	-0.066308	3.747266
341.556228	4807.453685	7.414042	-0.066397	3.750351
341.880084	4815.460203	7.419046	-0.066462	3.753419
342.308289	4823.481506	7.424051	-0.066547	3.756492
342.796220	4831.429654	7.429056	-0.066643	3.759537
342.935979	4839.503978	7.434061	-0.066675	3.762618
343.095080	4847.546052	7.439066	-0.066709	3.765685
343.024468	4855.612477	7.444070	-0.066702	3.768753
343.290081	4863.679994	7.449075	-0.066756	3.771828
343.848371	4871.601136	7.454080	-0.066865	3.774851
344.570062	4879.573825	7.459085	-0.067005	3.777895
344.534542	4887.703999	7.464090	-0.067004	3.780978
345.219472	4895.603417	7.469094	-0.067136	3.783988
345.806150	4903.669705	7.474099	-0.067251	3.787057
345.807863	4911.716031	7.479104	-0.067256	3.790102
346.042085	4919.785152	7.484109	-0.067305	3.793158
346.278788	4927.826846	7.489114	-0.067354	3.796202
346.461966	4935.793974	7.494118	-0.067394	3.799213
347.143378	4943.815110	7.499123	-0.067526	3.802255
347.290809	4951.755941	7.504128	-0.067558	3.805251
347.663430	4959.871983	7.509133	-0.067633	3.808316
347.843795	4967.924116	7.514138	-0.067672	3.811350
348.751200	4975.838688	7.519142	-0.067846	3.814346
349.189048	4983.904312	7.524147	-0.067933	3.817386
349.575877	4991.883084	7.529152	-0.068010	3.820389
349.961176	4999.925026	7.534157	-0.068087	3.823414
349.998026	5007.999945	7.539162	-0.068099	3.826441
349.567041	5016.108010	7.544166	-0.068024	3.829468
350.175149	5024.092012	7.549171	-0.068142	3.832469
350.238681	5032.096040	7.554176	-0.068160	3.835463
350.632686	5040.135567	7.559181	-0.068238	3.838475
350.841109	5048.135485	7.564186	-0.068282	3.841466
351.485231	5056.054528	7.569190	-0.068407	3.844434
352.102167	5064.106406	7.574195	-0.068527	3.847448
351.932918	5072.202571	7.579200	-0.068501	3.850460
351.959925	5080.275287	7.584205	-0.068511	3.853464
352.916826	5088.195339	7.589210	-0.068695	3.856429
352.641667	5096.236641	7.594214	-0.068649	3.859411
352.912802	5104.298466	7.599219	-0.068704	3.862410
353.274379	5112.276531	7.604224	-0.068777	3.865377
353.644164	5120.311825	7.609229	-0.068851	3.868363
354.063088	5128.365070	7.614234	-0.068934	3.871355
354.495097	5136.422315	7.619238	-0.069020	3.874346
354.906739	5144.460091	7.624243	-0.069102	3.877327
355.277140	5152.364534	7.629248	-0.069176	3.880255
356.057331	5160.330235	7.634253	-0.069326	3.883212
356.326795	5168.420274	7.639258	-0.069382	3.886202
356.527608	5176.423866	7.644262	-0.069424	3.889157
356.772200	5184.471935	7.649267	-0.069475	3.892127
357.372741	5192.432160	7.654272	-0.069592	3.895069
357.956591	5200.423353	7.659277	-0.069706	3.898020
358.105829	5208.514107	7.664282	-0.069739	3.900996
358.641084	5216.466945	7.669286	-0.069844	3.903928
358.585477	5224.632275	7.674291	-0.069839	3.906923
358.583779	5232.590583	7.679296	-0.069844	3.909841
359.240613	5240.590401	7.684301	-0.069971	3.912785
359.108092	5248.687182	7.689306	-0.069952	3.915747
359.203339	5256.672105	7.694310	-0.069975	3.918670
359.478645	5264.739810	7.699315	-0.070031	3.921625
360.034405	5272.620269	7.704320	-0.070140	3.924514
360.065833	5280.769578	7.709325	-0.070151	3.927489
360.429908	5288.767276	7.714330	-0.070224	3.930413
360.752335	5296.740699	7.719334	-0.070289	3.933326
361.091612	5304.824781	7.724339	-0.070358	3.936276
361.351072	5312.771597	7.729344	-0.070411	3.939173
361.662447	5320.841086	7.734349	-0.070474	3.942113
361.749160	5328.891304	7.739354	-0.070496	3.945040
361.972969	5336.896675	7.744358	-0.070542	3.947951
362.749804	5344.900572	7.749363	-0.070692	3.950870
363.133862	5352.892737	7.754368	-0.070769	3.953774
363.373720	5360.975817	7.759373	-0.070819	3.956707
363.406517	5368.973622	7.764378	-0.070830	3.959603
363.500362	5376.984604	7.769382	-0.070853	3.962503
364.164561	5384.968714	7.774387	-0.070982	3.965401
364.852612	5392.934426	7.779392	-0.071115	3.968291
364.737473	5401.080133	7.784397	-0.071099	3.971229
365.391080	5409.044114	7.789402	-0.071226	3.974113
365.957864	5417.053093	7.794406	-0.071337	3.977010
366.391452	5425.040857	7.799411	-0.071422	3.979894
366.661032	5433.075577	7.804416	-0.071478	3.982790
366.724523	5441.166221	7.809421	-0.071495	3.985701
367.054142	5449.157823	7.814426	-0.071562	3.988579
367.030885	5457.257567	7.819430	-0.071562	3.991487
367.385634	5465.210184	7.824435	-0.071634	3.994346
367.949379	5473.197001	7.829440	-0.071744	3.997220
368.292679	5481.202038	7.834445	-0.071813	4.000094
368.433288	5489.250499	7.839450	-0.071844	4.002978
368.920951	5497.222993	7.844454	-0.071940	4.005839
369.228525	5505.277996	7.849459	-0.072003	4.008724
369.335448	5513.302868	7.854464	-0.072028	4.011593
369.730308	5521.367364	7.859469	-0.072107	4.014478
369.743785	5529.428390	7.864474	-0.072114	4.017354
370.168533	5537.336914	7.869478	-0.072199	4.020181
370.471879	5545.372497	7.874483	-0.072260	4.023048
370.855637	5553.383069	7.879488	-0.072337	4.025906
370.904852	5561.450754	7.884493	-0.072351	4.028777
371.291821	5569.516793	7.889498	-0.072429	4.031650
371.247987	5577.589771	7.894502	-0.072426	4.034517
371.568562	5585.605446	7.899507	-0.072491	4.037368
371.815291	5593.551875	7.904512	-0.072542	4.040190
372.317728	5601.517231	7.909517	-0.072641	4.043022
372.379175	5609.525616	7.914522	-0.072657	4.045859
372.472426	5617.541780	7.919526	-0.072680	4.048698
373.125693	5625.565443	7.924531	-0.072807	4.051546
373.383166	5633.555837	7.929536	-0.072860	4.054374
373.271722	5641.686513	7.934541	-0.072844	4.057245
373.551010	5649.679397	7.939546	-0.072901	4.060070
373.685272	5657.670079	7.944550	-0.072932	4.062890
373.824682	5665.731725	7.949555	-0.072963	4.065734
373.962397	5673.753931	7.954560	-0.072994	4.068561
374.248469	5681.829581	7.959565	-0.073052	4.071408
374.464531	5689.810092	7.964570	-0.073098	4.074218
374.439524	5697.825952	7.969574	-0.073098	4.077035
374.818153	5705.834812	7.974579	-0.073174	4.079854
375.055684	5713.789441	7.979584	-0.073223	4.082649
375.491251	5721.817947	7.984589	-0.073310	4.085471
375.452926	5729.888791	7.989594	-0.073308	4.088300
375.800768	5737.891307	7.994598	-0.073378	4.091108
376.262697	5745.895676	7.999603	-0.073469	4.093916
376.700902	5753.881711	8.004608	-0.073556	4.096715
376.904261	5761.906193	8.009613	-0.073599	4.099523
377.055269	5769.977732	8.014618	-0.073632	4.102344
377.552265	5777.940733	8.019622	-0.073730	4.105131
377.685047	5786.009930	8.024627	-0.073760	4.107947
377.832036	5794.054593	8.029632	-0.073792	4.110753
378.020553	5802.045787	8.034637	-0.073833	4.113539
378.950812	5810.040075	8.039642	-0.074011	4.116335
379.304879	5817.985645	8.044646	-0.074082	4.119103
379.571705	5826.088380	8.049651	-0.074137	4.121923
379.669647	5834.021743	8.054656	-0.074161	4.124680
379.813871	5842.160202	8.059661	-0.074193	4.127507
380.181015	5850.141757	8.064666	-0.074266	4.130281
380.100008	5858.199186	8.069670	-0.074256	4.133073
380.449738	5866.238383	8.074675	-0.074327	4.135862
380.684945	5874.190979	8.079680	-0.074376	4.138619
380.928170	5882.225412	8.084685	-0.074426	4.141401
381.086674	5890.183625	8.089690	-0.074461	4.144155
381.038401	5898.312226	8.094694	-0.074457	4.146962
382.115046	5906.174718	8.099699	-0.074663	4.149690
382.033884	5914.261281	8.104704	-0.074653	4.152479
382.205180	5922.352117	8.109709	-0.074690	4.155271
382.037028	5930.404699	8.114714	-0.074664	4.158043
382.884992	5938.355755	8.119718	-0.074827	4.160792
383.158771	5946.335942	8.124723	-0.074883	4.163541
383.103161	5954.405141	8.129728	-0.074878	4.166315
383.357624	5962.394976	8.134733	-0.074931	4.169063
383.860965	5970.461363	8.139738	-0.075030	4.171840
384.048340	5978.434414	8.144742	-0.075070	4.174578
384.562089	5986.468677	8.149747	-0.075171	4.177339
384.463611	5994.502588	8.154752	-0.075157	4.180091
384.515454	6002.522844	8.159757	-0.075172	4.182839
384.745813	6010.550429	8.164762	-0.075220	4.185589
384.651866	6018.577221	8.169766	-0.075208	4.188333
384.578389	6026.676159	8.174771	-0.075200	4.191100
385.166670	6034.666454	8.179776	-0.075314	4.193837
385.307557	6042.702988	8.184781	-0.075346	4.196581
385.768535	6050.574769	8.189786	-0.075437	4.199272
386.137053	6058.635365	8.194790	-0.075511	4.202024
386.445652	6066.599809	8.199795	-0.075573	4.204741
386.394851	6074.672245	8.204800	-0.075569	4.207488
386.906783	6082.664427	8.209805	-0.075670	4.210213
387.220466	6090.718087	8.214810	-0.075733	4.212955
387.156814	6098.712186	8.219814	-0.075727	4.215671
387.156810	6106.770066	8.224819	-0.075732	4.218407
387.425875	6114.779450	8.229824	-0.075787	4.221128
387.816950	6122.765360	8.234829	-0.075865	4.223840
388.250482	6130.821576	8.239834	-0.075951	4.226575
388.160772	6138.820386	8.244838	-0.075940	4.229283
388.611808	6146.883016	8.249843	-0.076029	4.232016
388.951798	6154.830784	8.254848	-0.076097	4.234708
389.105392	6162.934577	8.259853	-0.076131	4.237449
389.312424	6170.905215	8.264858	-0.076175	4.240144
389.128539	6178.939212	8.269862	-0.076146	4.242854
389.684475	6186.971562	8.274867	-0.076255	4.245569
389.378127	6194.978786	8.279872	-0.076203	4.248266
389.782954	6203.032702	8.284877	-0.076283	4.250984
390.094535	6210.998262	8.289882	-0.076347	4.253669
390.347154	6219.013424	8.294886	-0.076399	4.256368
390.512100	6227.040077	8.299891	-0.076435	4.259069
390.783356	6235.029767	8.304896	-0.076490	4.261757
391.228925	6242.970283	8.309901	-0.076579	4.264428
391.487526	6251.110235	8.314906	-0.076632	4.267163
391.616986	6259.065552	8.319910	-0.076661	4.269832
391.552138	6267.176763	8.324915	-0.076654	4.272551
391.978235	6275.096555	8.329920	-0.076739	4.275208
391.779814	6283.151818	8.334925	-0.076707	4.277903
392.456128	6291.162557	8.339930	-0.076838	4.280589
392.800183	6299.101857	8.344934	-0.076908	4.283247
393.453400	6307.154586	8.349939	-0.077034	4.285944
393.567008	6315.162821	8.354944	-0.077061	4.288619
393.768801	6323.275729	8.359949	-0.077104	4.291328
394.300453	6331.247354	8.364954	-0.077208	4.293992
394.094320	6339.260668	8.369958	-0.077175	4.296661
394.257052	6347.290699	8.374963	-0.077210	4.299337
394.512367	6355.329007	8.379968	-0.077263	4.302015
394.815802	6363.309224	8.384973	-0.077325	4.304672
394.713386	6371.360416	8.389978	-0.077311	4.307348
395.319070	6379.333558	8.394982	-0.077429	4.310002
395.363781	6387.423024	8.399987	-0.077442	4.312689
396.028309	6395.350383	8.404992	-0.077571	4.315325
396.374507	6403.313446	8.409997	-0.077641	4.317969
396.986404	6411.315446	8.415002	-0.077760	4.320626
397.202293	6419.315428	8.420006	-0.077805	4.323278
396.956887	6427.463794	8.425011	-0.077765	4.325973
396.936754	6435.456856	8.430016	-0.077766	4.328617
397.466298	6443.506741	8.435021	-0.077870	4.331282
397.522722	6451.483317	8.440026	-0.077886	4.333918
397.799669	6459.516301	8.445030	-0.077943	4.336573
398.002122	6467.515383	8.450035	-0.077986	4.339214
398.547060	6475.508604	8.455040	-0.078092	4.341854
398.812779	6483.493474	8.460045	-0.078147	4.344488
399.007620	6491.609133	8.465050	-0.078188	4.347163
399.187063	6499.587920	8.470054	-0.078227	4.349791
399.625138	6507.655969	8.475059	-0.078314	4.352448
399.416263	6515.659040	8.480064	-0.078280	4.355078
399.694549	6523.638980	8.485069	-0.078337	4.357702
399.997383	6531.686079	8.490074	-0.078399	4.360346
400.207523	6539.614596	8.495078	-0.078443	4.362950
401.217309	6547.642115	8.500083	-0.078636	4.365590
400.996688	6555.700229	8.505088	-0.078600	4.368229
401.335798	6563.735086	8.510093	-0.078669	4.370864
401.480063	6571.749447	8.515098	-0.078701	4.373488
401.498623	6579.802798	8.520102	-0.078710	4.376123
401.850552	6587.797809	8.525107	-0.078780	4.378740
402.543313	6595.772649	8.530112	-0.078915	4.381351
402.620895	6603.774508	8.535117	-0.078934	4.383964
402.601686	6611.870187	8.540122	-0.078936	4.386606
402.596092	6619.878566	8.545126	-0.078940	4.389219
402.679329	6627.971410	8.550131	-0.078961	4.391857
403.164133	6635.877328	8.555136	-0.079056	4.394436
403.285841	6643.921669	8.560141	-0.079084	4.397056
403.451182	6651.932607	8.565146	-0.079120	4.399664
404.027827	6659.901262	8.570151	-0.079233	4.402259
404.541913	6667.906770	8.575155	-0.079334	4.404864
404.503135	6675.994716	8.580160	-0.079332	4.407491
404.889800	6683.997955	8.585165	-0.079409	4.410091
404.913412	6692.105034	8.590170	-0.079418	4.412721
405.177150	6700.042203	8.595175	-0.079473	4.415296
405.492127	6708.122959	8.600179	-0.079537	4.417917
405.448185	6716.174403	8.605184	-0.079534	4.420524
405.799414	6724.152375	8.610189	-0.079604	4.423108
406.129248	6732.179936	8.615194	-0.079671	4.425706
406.368080	6740.182009	8.620199	-0.079720	4.428295
407.063879	6748.217021	8.625203	-0.079855	4.430894
406.862441	6756.236020	8.630208	-0.079823	4.433482
407.099308	6764.267987	8.635213	-0.079872	4.436076
407.234915	6772.286049	8.640218	-0.079903	4.438662
406.920330	6780.378973	8.645223	-0.079849	4.441269
407.739142	6788.260994	8.650227	-0.080007	4.443812
408.225709	6796.299482	8.655232	-0.080103	4.446402
408.280742	6804.351398	8.660237	-0.080118	4.448993
408.601315	6812.360327	8.665242	-0.080183	4.451570
408.115970	6820.400614	8.670247	-0.080098	4.454152
408.777627	6828.384762	8.675251	-0.080226	4.456719
408.370330	6836.394158	8.680256	-0.080156	4.459289
409.097787	6844.411245	8.685261	-0.080296	4.461864
409.304939	6852.385089	8.690266	-0.080340	4.464421
409.502370	6860.396866	8.695271	-0.080382	4.466990
410.102985	6868.440961	8.700275	-0.080499	4.469568
410.083962	6876.506137	8.705280	-0.080501	4.472150
410.423171	6884.437447	8.710285	-0.080569	4.474688
410.677787	6892.480990	8.715290	-0.080622	4.477261
410.910265	6900.471887	8.720295	-0.080670	4.479815
410.935437	6908.560060	8.725299	-0.080680	4.482398
411.222849	6916.499908	8.730304	-0.080739	4.484933
411.258412	6924.612950	8.735309	-0.080751	4.487521
410.836252	6932.714710	8.740314	-0.080678	4.490101
411.252984	6940.608027	8.745319	-0.080760	4.492618
411.590514	6948.622605	8.750323	-0.080828	4.495171
411.394678	6956.680441	8.755328	-0.080797	4.497734
411.435144	6964.702801	8.760333	-0.080810	4.500286
412.137805	6972.626049	8.765338	-0.080946	4.502807
411.932945	6980.672130	8.770343	-0.080913	4.505362
412.417678	6988.695589	8.775347	-0.081008	4.507912
411.930210	6996.758700	8.780352	-0.080923	4.510468
412.050976	7004.720416	8.785357	-0.080951	4.512994
412.563311	7012.717131	8.790362	-0.081051	4.515530
413.005798	7020.707423	8.795367	-0.081139	4.518063
413.482377	7028.732624	8.800371	-0.081233	4.520605
413.610195	7036.753066	8.805376	-0.081262	4.523143
413.952863	7044.811596	8.810381	-0.081331	4.525693
413.812206	7052.890144	8.815386	-0.081310	4.528245
413.916384	7060.853344	8.820391	-0.081334	4.530761
414.625636	7068.824570	8.825395	-0.081472	4.533280
414.717838	7076.766262	8.830400	-0.081494	4.535786
415.112147	7084.838576	8.835405	-0.081573	4.538332
415.169709	7092.954040	8.840410	-0.081589	4.540890
415.514369	7100.862605	8.845415	-0.081658	4.543382
415.715216	7108.923598	8.850419	-0.081700	4.545920
416.297996	7116.876084	8.855424	-0.081814	4.548424
416.335339	7124.952462	8.860429	-0.081826	4.550964
416.385858	7132.961736	8.865434	-0.081841	4.553481
416.083255	7141.044582	8.870439	-0.081790	4.556019
416.386540	7149.015243	8.875443	-0.081852	4.558522
416.420460	7157.043971	8.880448	-0.081863	4.561041
416.579528	7164.990701	8.885453	-0.081898	4.563533
416.725196	7173.068474	8.890458	-0.081930	4.566065
417.464624	7180.943787	8.895463	-0.082073	4.568534
417.346869	7189.125986	8.900467	-0.082056	4.571095
417.491904	7197.077682	8.905472	-0.082089	4.573583
417.989070	7205.096740	8.910477	-0.082186	4.576092
417.873881	7213.099681	8.915482	-0.082170	4.578593
418.519593	7221.081062	8.920487	-0.082296	4.581087
418.962351	7229.091064	8.925491	-0.082383	4.583588
418.600011	7237.227537	8.930496	-0.082321	4.586126
418.446105	7245.229243	8.935501	-0.082298	4.588622
418.884314	7253.236684	8.940506	-0.082384	4.591118
418.859866	7261.212490	8.945511	-0.082385	4.593602
419.173380	7269.299603	8.950515	-0.082449	4.596121
419.556908	7277.181266	8.955520	-0.082525	4.598574
419.647312	7285.262140	8.960525	-0.082547	4.601087
419.835965	7293.214524	8.965530	-0.082587	4.603559
419.751884	7301.296781	8.970535	-0.082577	4.606070
420.099272	7309.286585	8.975539	-0.082647	4.608551
420.586211	7317.293533	8.980544	-0.082743	4.611036
420.264391	7325.350390	8.985549	-0.082688	4.613534
420.976621	7333.361669	8.990554	-0.082826	4.616018
420.764768	7341.347328	8.995559	-0.082792	4.618492
421.045662	7349.412854	9.000563	-0.082849	4.620990
421.034056	7357.394591	9.005568	-0.082852	4.623460
421.099295	7365.472351	9.010573	-0.082870	4.625958
421.454641	7373.464195	9.015578	-0.082941	4.628429
421.275336	7381.462121	9.020583	-0.082913	4.630900
421.495991	7389.462834	9.025587	-0.082959	4.633371
422.101489	7397.466577	9.030592	-0.083077	4.635841
422.078030	7405.496496	9.035597	-0.083078	4.638318
422.463658	7413.579144	9.040602	-0.083155	4.640810
422.428586	7421.506274	9.045607	-0.083154	4.643253
422.214526	7429.583596	9.050611	-0.083119	4.645740
422.662941	7437.512071	9.055616	-0.083208	4.648181
423.126694	7445.578890	9.060621	-0.083299	4.650663
423.052256	7453.608279	9.065626	-0.083291	4.653132
423.290435	7461.587266	9.070631	-0.083340	4.655584
423.788431	7469.601301	9.075635	-0.083438	4.658045
423.738038	7477.617129	9.080640	-0.083434	4.660506
424.152757	7485.576724	9.085645	-0.083516	4.662948
424.547615	7493.634319	9.090650	-0.083595	4.665418
424.602306	7501.746711	9.095655	-0.083610	4.667905
424.544810	7509.808195	9.100659	-0.083605	4.670374
424.453092	7517.804501	9.105664	-0.083593	4.672823
424.584573	7525.818752	9.110669	-0.083623	4.675275
425.201857	7533.771088	9.115674	-0.083743	4.677707
425.190983	7541.783333	9.120679	-0.083746	4.680156
425.648076	7549.739798	9.125683	-0.083836	4.682586
425.853124	7557.745826	9.130688	-0.083880	4.685031
426.222245	7565.768939	9.135693	-0.083954	4.687479
426.487406	7573.778634	9.140698	-0.084008	4.689922
426.874521	7581.855544	9.145703	-0.084086	4.692384
427.162192	7589.796069	9.150707	-0.084144	4.694803
427.376986	7597.824593	9.155712	-0.084190	4.697248
427.861924	7605.842125	9.160717	-0.084285	4.699688
427.544073	7613.954885	9.165722	-0.084231	4.702157
427.152442	7621.919456	9.170727	-0.084163	4.704579
427.351742	7630.063468	9.175731	-0.084206	4.707054
427.627132	7637.950077	9.180736	-0.084262	4.709449
427.955777	7645.965553	9.185741	-0.084329	4.711882
428.079753	7653.953324	9.190746	-0.084357	4.714306
428.292907	7662.031224	9.195751	-0.084402	4.716755
428.797965	7670.003848	9.200755	-0.084501	4.719171
429.083810	7678.002120	9.205760	-0.084559	4.721594
429.369908	7685.958211	9.210765	-0.084618	4.724002
429.077098	7694.146938	9.215770	-0.084569	4.726481
429.401947	7702.079645	9.220775	-0.084634	4.728880
429.721139	7710.161081	9.225779	-0.084699	4.731323
429.707453	7718.153557	9.230784	-0.084702	4.733738
429.904289	7726.222972	9.235789	-0.084744	4.736175
430.507976	7734.115488	9.240794	-0.084861	4.738556
430.723565	7742.156249	9.245799	-0.084906	4.740981
430.877997	7750.155178	9.250803	-0.084940	4.743393
431.037001	7758.210088	9.255808	-0.084975	4.745820
431.426102	7766.228566	9.260813	-0.085053	4.748235
431.973314	7774.268164	9.265818	-0.085160	4.750654
431.750613	7782.231816	9.270823	-0.085124	4.753051
432.165565	7790.304660	9.275827	-0.085206	4.755478
432.070332	7798.316984	9.280832	-0.085194	4.757887
431.938969	7806.352757	9.285837	-0.085174	4.760302
432.431042	7814.322478	9.290842	-0.085271	4.762694
432.622660	7822.325791	9.295847	-0.085312	4.765096
432.437499	7830.402423	9.300851	-0.085283	4.767520
432.502937	7838.408522	9.305856	-0.085300	4.769920
432.697510	7846.390818	9.310861	-0.085342	4.772312
433.126530	7854.396296	9.315866	-0.085427	4.774709
433.184888	7862.404164	9.320871	-0.085443	4.777106
433.355263	7870.428762	9.325875	-0.085480	4.779507
433.816070	7878.454367	9.330880	-0.085571	4.781906
434.411718	7886.308101	9.335885	-0.085687	4.784252
434.406861	7894.517628	9.340890	-0.085691	4.786705
434.751540	7902.458283	9.345895	-0.085761	4.789075
435.016987	7910.550647	9.350899	-0.085815	4.791489
434.991302	7918.498250	9.355904	-0.085816	4.793860
435.196892	7926.626421	9.360909	-0.085859	4.796283
435.480611	7934.558573	9.365914	-0.085917	4.798647
435.578870	7942.558484	9.370919	-0.085941	4.801029
435.499662	7950.543387	9.375923	-0.085931	4.803407
435.893978	7958.568740	9.380928	-0.086010	4.805794
436.284116	7966.620235	9.385933	-0.086088	4.808187
435.979708	7974.709770	9.390938	-0.086036	4.810593
436.006004	7982.671068	9.395943	-0.086046	4.812959
436.724880	7990.108449	9.400947	-0.086185	4.815165
437.142745	7994.833710	9.405952	-0.086266	4.816566

437.136728	7997.521073	9.410957	-0.086266	4.817364
437.177902	7998.851329	9.415962	-0.086275	4.817758
437.078747	7999.226580	9.420967	-0.086257	4.817870
437.062013	8000.335230	9.425971	-0.086254	4.818199
437.092013	8000.381938	9.430976	-0.086260	4.818213
437.616023	8000.259796	9.435981	-0.086357	4.818174
437.498163	8000.290775	9.440986	-0.086335	4.818184
437.728834	8000.249785	9.445991	-0.086378	4.818171
437.932943	8000.343098	9.450995	-0.086416	4.818198
438.230190	8000.203080	9.456000	-0.086472	4.818155
438.242624	8000.253754	9.461005	-0.086474	4.818170
438.470031	8000.322141	9.466010	-0.086516	4.818189
438.536094	8000.259928	9.471015	-0.086529	4.818171
438.762922	8000.284118	9.476019	-0.086571	4.818177
439.059666	8000.228263	9.481024	-0.086626	4.818159
438.903152	8000.239768	9.486029	-0.086597	4.818163
438.900319	8000.266031	9.491034	-0.086596	4.818171
438.735592	8000.183780	9.496039	-0.086566	4.818147
438.828734	8000.289234	9.501043	-0.086583	4.818178
439.356969	8000.217655	9.506048	-0.086681	4.818155
439.594298	8000.160975	9.511053	-0.086725	4.818137
439.515151	8000.224057	9.516058	-0.086711	4.818156
439.169124	8000.233982	9.521063	-0.086646	4.818160
438.973066	8000.285971	9.526067	-0.086610	4.818177
439.523002	8000.316753	9.531072	-0.086712	4.818183
439.129525	8000.335487	9.536077	-0.086639	4.818191
439.177516	8000.331944	9.541082	-0.086648	4.818189
439.408385	8000.219411	9.546087	-0.086691	4.818155
439.625181	8000.265558	9.551091	-0.086731	4.818168
439.753886	8000.270501	9.556096	-0.086755	4.818169
439.418789	8000.256377	9.561101	-0.086693	4.818166
439.469032	8000.298108	9.566106	-0.086702	4.818178
439.444401	8000.234635	9.571111	-0.086697	4.818159
439.563476	8000.310991	9.576115	-0.086720	4.818182
439.808278	8000.244946	9.581120	-0.086765	4.818161
439.814741	8000.219782	9.586125	-0.086766	4.818153
439.896575	8000.277735	9.591130	-0.086782	4.818170
439.752265	8000.230486	9.596135	-0.086755	4.818157
440.127358	8000.259894	9.601139	-0.086824	4.818164
440.076010	8000.254971	9.606144	-0.086815	4.818163
440.353572	8000.185173	9.611149	-0.086866	4.818141
440.384105	8000.259248	9.616154	-0.086872	4.818163
440.032529	8000.282772	9.621159	-0.086807	4.818171
440.183629	8000.296444	9.626163	-0.086835	4.818175
440.162643	8000.224603	9.631168	-0.086831	4.818153
440.591556	8000.266334	9.636173	-0.086911	4.818164
440.452946	8000.222320	9.641178	-0.086885	4.818152
440.664154	8000.188426	9.646183	-0.086924	4.818141
440.682138	8000.240232	9.651187	-0.086928	4.818156
440.240518	8000.256192	9.656192	-0.086845	4.818162
440.279324	8000.301973	9.661197	-0.086853	4.818176
440.393045	8000.276195	9.666202	-0.086874	4.818168
440.266955	8000.233407	9.671207	-0.086850	4.818156
440.723320	8000.291303	9.676211	-0.086935	4.818171
440.467057	8000.268802	9.681216	-0.086887	4.818165
440.554747	8000.255289	9.686221	-0.086904	4.818161
440.453537	8000.304386	9.691226	-0.086885	4.818176
440.123774	8000.293491	9.696231	-0.086823	4.818174
440.160591	8000.383437	9.701235	-0.086830	4.818201
440.475165	8000.353084	9.706240	-0.086889	4.818190
440.126840	8000.360870	9.711245	-0.086824	4.818194
440.038505	8000.474329	9.716250	-0.086808	4.818228
440.197500	8000.417615	9.721255	-0.086837	4.818211
439.828989	8000.489303	9.726259	-0.086769	4.818233
439.913001	8000.433651	9.731264	-0.086784	4.818216
440.202035	8000.379795	9.736269	-0.086838	4.818199
440.295272	8000.368463	9.741274	-0.086855	4.818196
440.481506	8000.268987	9.746279	-0.086890	4.818165
440.550122	8000.330966	9.751283	-0.086903	4.818183
440.553994	8000.357323	9.756288	-0.086903	4.818191
440.551978	8000.344668	9.761293	-0.086903	4.818187
440.435976	8000.353577	9.766298	-0.086881	4.818191
440.248625	8000.358338	9.771303	-0.086847	4.818193
440.202538	8000.421880	9.776307	-0.086838	4.818212
440.156155	8000.405451	9.781312	-0.086829	4.818207
440.421990	8000.408092	9.786317	-0.086879	4.818207
440.663916	8000.459853	9.791322	-0.086924	4.818221
440.591217	8000.387292	9.796327	-0.086910	4.818200
440.875394	8000.343891	9.801331	-0.086963	4.818186
440.927954	8000.322524	9.806336	-0.086973	4.818179
440.960240	8000.299823	9.811341	-0.086979	4.818172
440.717706	8000.426924	9.816346	-0.086934	4.818211
440.891716	8000.362001	9.821351	-0.086966	4.818191
441.073467	8000.330855	9.826355	-0.087000	4.818181
441.165856	8000.232178	9.831360	-0.087017	4.818152
441.228529	8000.300389	9.836365	-0.087029	4.818172
441.568544	8000.276704	9.841370	-0.087092	4.818163
441.472173	8000.245901	9.846375	-0.087074	4.818154
441.392893	8000.286886	9.851379	-0.087059	4.818167
441.854139	8000.297506	9.856384	-0.087145	4.818168
441.677871	8000.264540	9.861389	-0.087112	4.818159
441.413354	8000.339778	9.866394	-0.087063	4.818182
441.173637	8000.395368	9.871399	-0.087018	4.818200
441.215198	8000.447503	9.876403	-0.087026	4.818215
441.229152	8000.333005	9.881408	-0.087029	4.818181
441.819215	8000.246506	9.886413	-0.087139	4.818153
441.991067	8000.274147	9.891418	-0.087171	4.818161
441.983731	8000.224590	9.896423	-0.087169	4.818146
442.302311	8000.232174	9.901427	-0.087228	4.818147
441.948059	8000.256710	9.906432	-0.087162	4.818156
441.673272	8000.242367	9.911437	-0.087111	4.818152
441.897600	8000.262320	9.916442	-0.087153	4.818157
441.797490	8000.236726	9.921447	-0.087134	4.818150
442.062070	8000.283544	9.926451	-0.087184	4.818163
441.848493	8000.251111	9.931456	-0.087144	4.818154
442.100645	8000.195691	9.936461	-0.087191	4.818137
442.296027	8000.297315	9.941466	-0.087227	4.818166
442.247404	8000.247183	9.946471	-0.087218	4.818152
442.472688	8000.233479	9.951475	-0.087260	4.818147
442.077554	8000.261655	9.956480	-0.087186	4.818157
442.183282	8000.304161	9.961485	-0.087206	4.818169
441.750735	8000.347600	9.966490	-0.087126	4.818183
442.223276	8000.230006	9.971495	-0.087213	4.818147
442.263078	8000.275804	9.976499	-0.087221	4.818160
442.115248	8000.246390	9.981504	-0.087193	4.818152
442.418687	8000.193787	9.986509	-0.087250	4.818135
442.499925	8000.242266	9.991514	-0.087265	4.818149
442.079595	8000.238525	9.996519	-0.087187	4.818150
442.245205	8000.268184	10.001523	-0.087217	4.818158
442.094772	8000.278718	10.006528	-0.087189	4.818162
441.829695	8000.304494	10.011533	-0.087140	4.818170
441.889350	8000.351620	10.016538	-0.087151	4.818184
442.144625	8000.257310	10.021543	-0.087199	4.818155
442.637553	8000.228387	10.026547	-0.087290	4.818144
442.069364	8000.238374	10.031552	-0.087185	4.818150
442.349966	8000.243326	10.036557	-0.087237	4.818150
442.766506	8000.212289	10.041562	-0.087314	4.818139
442.456191	8000.183771	10.046567	-0.087257	4.818132
442.115888	8000.294784	10.051571	-0.087193	4.818166
442.120348	8000.243285	10.056576	-0.087194	4.818151
442.463654	8000.237535	10.061581	-0.087258	4.818148
442.312680	8000.253323	10.066586	-0.087230	4.818153
442.405071	8000.198838	10.071591	-0.087247	4.818137
442.288997	8000.258252	10.076595	-0.087225	4.818155
442.412620	8000.203149	10.081600	-0.087248	4.818138
442.650233	8000.214870	10.086605	-0.087293	4.818140
442.787194	8000.240975	10.091610	-0.087318	4.818147
442.743343	8000.189856	10.096615	-0.087310	4.818133
442.971825	8000.205659	10.101619	-0.087352	4.818136
442.673097	8000.189929	10.106624	-0.087297	4.818133
442.844489	8000.214408	10.111629	-0.087329	4.818139
442.953509	8000.229602	10.116634	-0.087349	4.818143
443.093806	8000.215769	10.121639	-0.087375	4.818139
443.069581	8000.245946	10.126643	-0.087371	4.818148
443.371672	8000.189116	10.131648	-0.087427	4.818130
443.014575	8000.188357	10.136653	-0.087360	4.818131
443.284990	8000.199483	10.141658	-0.087411	4.818133
442.896022	8000.202490	10.146663	-0.087338	4.818136
443.312770	8000.201971	10.151667	-0.087416	4.818134
442.719669	8000.233706	10.156672	-0.087305	4.818146
442.754227	8000.280484	10.161677	-0.087312	4.818159
443.598603	8000.184898	10.166682	-0.087469	4.818128
443.157869	8000.172453	10.171687	-0.087387	4.818126
443.266325	8000.213946	10.176691	-0.087407	4.818137
443.142444	8000.213274	10.181696	-0.087384	4.818138
443.362296	8000.150039	10.186701	-0.087425	4.818118
443.368076	8000.215358	10.191706	-0.087426	4.818137
443.377795	8000.188133	10.196711	-0.087428	4.818129
443.244055	8000.219944	10.201715	-0.087403	4.818139
443.365729	8000.197433	10.206720	-0.087425	4.818132
443.125195	8000.217236	10.211725	-0.087381	4.818139
442.774086	8000.301792	10.216730	-0.087315	4.818166
442.916884	8000.232224	10.221735	-0.087342	4.818144
443.152065	8000.250225	10.226739	-0.087386	4.818149
443.223303	8000.236484	10.231744	-0.087399	4.818144
443.138202	8000.234246	10.236749	-0.087383	4.818144
443.452488	8000.211258	10.241754	-0.087441	4.818136
443.257362	8000.191707	10.246759	-0.087405	4.818131
443.834110	8000.181840	10.251763	-0.087512	4.818126
443.530695	8000.217604	10.256768	-0.087456	4.818137
443.933691	8000.164283	10.261773	-0.087531	4.818120
443.712038	8000.208550	10.266778	-0.087490	4.818134
443.840998	8000.170357	10.271783	-0.087514	4.818122
443.882658	8000.194085	10.276787	-0.087521	4.818129
443.898824	8000.196413	10.281792	-0.087524	4.818130
443.779004	8000.203163	10.286797	-0.087502	4.818132
443.730228	8000.211953	10.291802	-0.087493	4.818135
443.983317	8000.188115	10.296807	-0.087540	4.818127
443.976343	8000.184859	10.301811	-0.087539	4.818126
443.685670	8000.188180	10.306816	-0.087485	4.818128
443.379267	8000.239686	10.311821	-0.087428	4.818145
443.614291	8000.257686	10.316826	-0.087471	4.818149
443.556582	8000.213739	10.321831	-0.087461	4.818136
443.928820	8000.205237	10.326835	-0.087530	4.818132
443.966955	8000.173147	10.331840	-0.087537	4.818123
443.772659	8000.200958	10.336845	-0.087501	4.818132
444.114853	8000.183620	10.341850	-0.087564	4.818125
444.445069	8000.130339	10.346855	-0.087626	4.818108
444.234433	8000.215798	10.351859	-0.087587	4.818134
444.102329	8000.184494	10.356864	-0.087562	4.818125
444.339505	8000.141494	10.361869	-0.087606	4.818112
444.242326	8000.191701	10.366874	-0.087588	4.818127
443.849672	8000.199916	10.371879	-0.087515	4.818131
444.478917	8000.176051	10.376883	-0.087632	4.818121
443.916875	8000.151392	10.381888	-0.087527	4.818116
444.470374	8000.122263	10.386893	-0.087630	4.818105
444.462637	8000.142147	10.391898	-0.087629	4.818111
444.519755	8000.120843	10.396903	-0.087640	4.818105
444.344928	8000.169971	10.401907	-0.087607	4.818120
444.110326	8000.201430	10.406912	-0.087563	4.818130
444.103244	8000.213957	10.411917	-0.087562	4.818134
444.191358	8000.228862	10.416922	-0.087578	4.818138
444.120125	8000.216294	10.421927	-0.087565	4.818135
444.119812	8000.196296	10.426931	-0.087565	4.818129
443.918449	8000.221904	10.431936	-0.087528	4.818137
444.060667	8000.213359	10.436941	-0.087554	4.818134
443.762567	8000.242882	10.441946	-0.087499	4.818144
443.557572	8000.228454	10.446951	-0.087460	4.818141
443.283291	8000.294086	10.451955	-0.087409	4.818161
443.525257	8000.244838	10.456960	-0.087454	4.818146
443.742126	8000.255220	10.461965	-0.087495	4.818148
443.879965	8000.255032	10.466970	-0.087520	4.818147
443.576433	8000.264487	10.471975	-0.087464	4.818151
443.775456	8000.238844	10.476979	-0.087501	4.818143
443.500890	8000.296054	10.481984	-0.087450	4.818161
443.629840	8000.275749	10.486989	-0.087474	4.818154
443.751856	8000.275341	10.491994	-0.087496	4.818154
443.447986	8000.246910	10.496999	-0.087440	4.818147
443.891171	8000.267807	10.502003	-0.087522	4.818151
443.156100	8000.277572	10.507008	-0.087385	4.818157
443.882957	8000.209815	10.512013	-0.087521	4.818134
443.849154	8000.221971	10.517018	-0.087514	4.818137
443.815906	8000.195201	10.522023	-0.087508	4.818130
443.830428	8000.248015	10.527027	-0.087511	4.818145
443.587907	8000.221490	10.532032	-0.087466	4.818138
443.606447	8000.249105	10.537037	-0.087469	4.818147
443.512149	8000.284621	10.542042	-0.087452	4.818157
443.542240	8000.290300	10.547047	-0.087457	4.818159
443.487604	8000.326368	10.552051	-0.087447	4.818170
443.260702	8000.328471	10.557056	-0.087405	4.818172
442.887493	8000.380099	10.562061	-0.087335	4.818188
443.008919	8000.398623	10.567066	-0.087358	4.818193
442.995391	8000.321619	10.572071	-0.087355	4.818171
443.260388	8000.338984	10.577075	-0.087405	4.818175
443.624272	8000.307216	10.582080	-0.087472	4.818164
444.120691	8000.208896	10.587085	-0.087565	4.818133
444.025174	8000.263336	10.592090	-0.087547	4.818149
444.364572	8000.176510	10.597095	-0.087610	4.818122
444.159137	8000.257832	10.602099	-0.087572	4.818147
444.061458	8000.256471	10.607104	-0.087554	4.818147
443.652049	8000.276028	10.612109	-0.087477	4.818154
444.046203	8000.263623	10.617114	-0.087551	4.818149
443.627439	8000.276735	10.622119	-0.087473	4.818155
443.322349	8000.327207	10.627123	-0.087416	4.818171
443.441701	8000.324657	10.632128	-0.087438	4.818170
443.538784	8000.307066	10.637133	-0.087456	4.818164
443.299873	8000.386869	10.642138	-0.087412	4.818189
443.298806	8000.342658	10.647143	-0.087412	4.818176
443.498686	8000.326497	10.652147	-0.087449	4.818170
443.532135	8000.345902	10.657152	-0.087455	4.818176
443.608802	8000.248055	10.662157	-0.087469	4.818146
443.465206	8000.356543	10.667162	-0.087443	4.818179
443.301215	8000.303752	10.672167	-0.087412	4.818164
443.547416	8000.301915	10.677171	-0.087458	4.818162
443.320051	8000.316639	10.682176	-0.087415	4.818168
443.227661	8000.285889	10.687181	-0.087398	4.818159
443.448194	8000.372085	10.692186	-0.087439	4.818184
443.200868	8000.341283	10.697191	-0.087393	4.818176
443.615044	8000.327052	10.702195	-0.087470	4.818170
444.074693	8000.225063	10.707200	-0.087556	4.818137
444.088337	8000.229461	10.712205	-0.087558	4.818139
443.826774	8000.254231	10.717210	-0.087510	4.818147
443.635664	8000.254728	10.722215	-0.087474	4.818148
443.603992	8000.286906	10.727219	-0.087468	4.818158
443.501995	8000.306531	10.732224	-0.087449	4.818164
443.602094	8000.295295	10.737229	-0.087468	4.818160
443.962016	8000.272943	10.742234	-0.087535	4.818152
443.549498	8000.357697	10.747239	-0.087458	4.818179
443.935667	8000.306247	10.752243	-0.087530	4.818162
443.983624	8000.297442	10.757248	-0.087539	4.818159
443.606715	8000.313242	10.762253	-0.087469	4.818166
443.743752	8000.362500	10.767258	-0.087494	4.818180
443.771401	8000.332367	10.772263	-0.087499	4.818171
443.701693	8000.333501	10.777267	-0.087486	4.818171
443.678341	8000.383683	10.782272	-0.087482	4.818186
443.351090	8000.403330	10.787277	-0.087421	4.818193
443.745533	8000.338316	10.792282	-0.087494	4.818172
443.463491	8000.345965	10.797287	-0.087442	4.818176
443.310975	8000.442755	10.802291	-0.087413	4.818205
443.342030	8000.412670	10.807296	-0.087419	4.818196
443.437031	8000.316130	10.812301	-0.087437	4.818167
443.143801	8000.421484	10.817306	-0.087382	4.818200
443.079040	8000.356394	10.822311	-0.087370	4.818181
442.950089	8000.427205	10.827315	-0.087346	4.818202
442.999148	8000.462610	10.832320	-0.087355	4.818212
443.524559	8000.419412	10.837325	-0.087453	4.818197
443.178812	8000.544028	10.842330	-0.087389	4.818236
443.026896	8000.454575	10.847335	-0.087360	4.818210
443.153041	8000.472113	10.852339	-0.087384	4.818215
443.336950	8000.423110	10.857344	-0.087418	4.818199
443.020470	8000.494468	10.862349	-0.087359	4.818222
443.400026	8000.446083	10.867354	-0.087430	4.818206
443.431418	8000.424421	10.872359	-0.087436	4.818199
443.599712	8000.390984	10.877363	-0.087467	4.818189
443.204657	8000.501235	10.882368	-0.087393	4.818223
443.393242	8000.403893	10.887373	-0.087428	4.818193
443.580190	8000.474891	10.892378	-0.087463	4.818214
443.140312	8000.457193	10.897383	-0.087381	4.818210
443.291732	8000.499285	10.902387	-0.087410	4.818222
443.355923	8000.418100	10.907392	-0.087421	4.818198
443.298791	8000.388893	10.912397	-0.087411	4.818189
443.480819	8000.428254	10.917402	-0.087445	4.818200
443.754399	8000.343669	10.922407	-0.087496	4.818174
444.021234	8000.374741	10.927411	-0.087545	4.818182
443.850038	8000.434441	10.932416	-0.087513	4.818201
443.851070	8000.389206	10.937421	-0.087514	4.818187
444.013721	8000.380946	10.942426	-0.087544	4.818184
443.953876	8000.348544	10.947431	-0.087533	4.818175
444.117357	8000.327667	10.952435	-0.087563	4.818168
444.510287	8000.305776	10.957440	-0.087636	4.818160
444.469704	8000.264171	10.962445	-0.087629	4.818147
444.226267	8000.319709	10.967450	-0.087583	4.818165
444.088585	8000.325158	10.972455	-0.087558	4.818167
444.226927	8000.286043	10.977459	-0.087583	4.818155
443.868644	8000.309467	10.982464	-0.087517	4.818163
444.046781	8000.293004	10.987469	-0.087550	4.818158
443.737521	8000.442331	10.992474	-0.087492	4.818203
443.362668	8000.484465	10.997479	-0.087422	4.818217
443.495312	8000.471578	11.002483	-0.087447	4.818213
443.361161	8000.516010	11.007488	-0.087422	4.818227
443.534382	8000.392147	11.012493	-0.087454	4.818189
443.603650	8000.492023	11.017498	-0.087467	4.818219
443.429017	8000.470650	11.022503	-0.087435	4.818213
443.455065	8000.448914	11.027507	-0.087440	4.818206
443.944339	8000.401004	11.032512	-0.087531	4.818190
443.865720	8000.343086	11.037517	-0.087516	4.818173
444.154089	8000.374457	11.042522	-0.087570	4.818182
443.579160	8000.453793	11.047527	-0.087463	4.818207
443.428610	8000.438017	11.052531	-0.087435	4.818203
443.500741	8000.453751	11.057536	-0.087448	4.818208
443.348928	8000.409547	11.062541	-0.087420	4.818195
443.664261	8000.431822	11.067546	-0.087478	4.818201
443.544395	8000.466982	11.072551	-0.087456	4.818211
443.444177	8000.457168	11.077555	-0.087437	4.818209
443.767617	8000.423787	11.082560	-0.087498	4.818198
443.678953	8000.421499	11.087565	-0.087481	4.818197
443.593043	8000.485543	11.092570	-0.087465	4.818217
443.338264	8000.488310	11.097575	-0.087418	4.818219
443.566306	8000.405196	11.102579	-0.087460	4.818193
443.672777	8000.489806	11.107584	-0.087480	4.818218
443.569187	8000.455743	11.112589	-0.087461	4.818208
443.794404	8000.446249	11.117594	-0.087502	4.818204
443.869921	8000.392580	11.122599	-0.087516	4.818188
444.165989	8000.439844	11.127603	-0.087572	4.818201
443.771837	8000.426990	11.132608	-0.087498	4.818199
443.395000	8000.392281	11.137613	-0.087428	4.818190
443.892426	8000.425509	11.142618	-0.087521	4.818198
444.218189	8000.326919	11.147623	-0.087581	4.818167
443.876002	8000.392657	11.152627	-0.087517	4.818188
443.943854	8000.403071	11.157632	-0.087530	4.818191
443.653673	8000.430599	11.162637	-0.087476	4.818200
443.828200	8000.442498	11.167642	-0.087509	4.818203
443.774467	8000.430174	11.172647	-0.087499	4.818200
443.839439	8000.455279	11.177651	-0.087511	4.818207
443.994605	8000.444810	11.182656	-0.087539	4.818203
443.776805	8000.451248	11.187661	-0.087499	4.818206
443.768893	8000.476391	11.192666	-0.087497	4.818213
443.668495	8000.458156	11.197671	-0.087479	4.818208
443.497942	8000.498925	11.202675	-0.087447	4.818221
443.583878	8000.522217	11.207680	-0.087463	4.818228
443.823965	8000.456108	11.212685	-0.087508	4.818207
443.788168	8000.484020	11.217690	-0.087501	4.818216
443.721078	8000.395746	11.222695	-0.087488	4.818190
443.913283	8000.461556	11.227699	-0.087524	4.818208
443.569389	8000.520957	11.232704	-0.087460	4.818227
443.595019	8000.468699	11.237709	-0.087465	4.818212
443.685123	8000.454168	11.242714	-0.087482	4.818207
443.517062	8000.501284	11.247719	-0.087450	4.818222
443.874069	8000.428384	11.252723	-0.087517	4.818199
444.105132	8000.410553	11.257728	-0.087560	4.818192
444.010168	8000.396603	11.262733	-0.087542	4.818189
443.946940	8000.492531	11.267738	-0.087530	4.818217
444.228451	8000.357547	11.272743	-0.087583	4.818176
444.528416	8000.354356	11.277747	-0.087639	4.818174
444.175918	8000.356813	11.282752	-0.087573	4.818176
443.641442	8000.450392	11.287757	-0.087473	4.818206
443.772220	8000.536393	11.292762	-0.087498	4.818231
443.735754	8000.501159	11.297767	-0.087491	4.818221
443.767266	8000.490022	11.302771	-0.087497	4.818217
443.590020	8000.511756	11.307776	-0.087464	4.818225
443.362315	8000.548572	11.312781	-0.087421	4.818236
443.507553	8000.470619	11.317786	-0.087448	4.818213
443.402930	8000.521775	11.322791	-0.087429	4.818228
443.546285	8000.517456	11.327795	-0.087456	4.818226
443.431677	8000.547428	11.332800	-0.087434	4.818236
443.200371	8000.565252	11.337805	-0.087391	4.818242
443.356480	8000.480085	11.342810	-0.087420	4.818216
443.482810	8000.534456	11.347815	-0.087444	4.818232
443.597578	8000.539209	11.352819	-0.087465	4.818233
443.526234	8000.543476	11.357824	-0.087452	4.818234
443.550808	8000.538556	11.362829	-0.087456	4.818233
443.579303	8000.431619	11.367834	-0.087462	4.818201
443.489841	8000.432477	11.372839	-0.087445	4.818201
443.767233	8000.441598	11.377843	-0.087497	4.818203
444.119500	8000.465441	11.382848	-0.087562	4.818209
443.956869	8000.443183	11.387853	-0.087532	4.818203
444.098903	8000.487250	11.392858	-0.087558	4.818215
443.830740	8000.481411	11.397863	-0.087508	4.818215
444.118587	8000.407548	11.402867	-0.087562	4.818192
444.202934	8000.376100	11.407872	-0.087578	4.818182
444.265630	8000.332776	11.412877	-0.087589	4.818169
444.569920	8000.381206	11.417882	-0.087646	4.818182
444.214500	8000.395199	11.422887	-0.087580	4.818187
444.293718	8000.452071	11.427891	-0.087594	4.818204
444.237631	8000.453394	11.432896	-0.087584	4.818205
444.254812	8000.405227	11.437901	-0.087587	4.818190
443.994054	8000.439478	11.442906	-0.087539	4.818201
444.234924	8000.403895	11.447911	-0.087583	4.818190
444.156868	8000.439637	11.452915	-0.087569	4.818201
444.084730	8000.431266	11.457920	-0.087555	4.818199
444.433882	8000.357204	11.462925	-0.087620	4.818175
444.784051	8000.396803	11.467930	-0.087686	4.818186
444.785284	8000.338943	11.472935	-0.087686	4.818168
444.354831	8000.412923	11.477939	-0.087606	4.818192
444.124226	8000.500208	11.482944	-0.087563	4.818219
444.283749	8000.382467	11.487949	-0.087592	4.818183
444.359618	8000.392992	11.492954	-0.087606	4.818186
444.677931	8000.297455	11.497959	-0.087666	4.818157
444.759014	8000.330151	11.502963	-0.087681	4.818166
444.877846	8000.326543	11.507968	-0.087703	4.818164
445.011908	8000.252643	11.512973	-0.087728	4.818142
444.932352	8000.297835	11.517978	-0.087713	4.818156
444.895060	8000.288896	11.522983	-0.087706	4.818153
444.505651	8000.358187	11.527987	-0.087633	4.818175
444.348985	8000.458077	11.532992	-0.087604	4.818206
444.242407	8000.409239	11.537997	-0.087584	4.818192
443.998288	8000.450035	11.543002	-0.087539	4.818205
444.248840	8000.357764	11.548007	-0.087586	4.818176
444.944205	8000.290626	11.553011	-0.087715	4.818153
445.079714	8000.252524	11.558016	-0.087740	4.818142
445.189591	8000.262471	11.563021	-0.087761	4.818144
445.101555	8000.320173	11.568026	-0.087744	4.818162
444.514327	8000.380395	11.573031	-0.087635	4.818182
444.356265	8000.400291	11.578035	-0.087606	4.818188
444.541411	8000.372351	11.583040	-0.087640	4.818179
444.525419	8000.340558	11.588045	-0.087637	4.818170
444.732342	8000.378164	11.593050	-0.087675	4.818180
444.732311	8000.322390	11.598055	-0.087675	4.818164
445.174822	8000.326446	11.603059	-0.087758	4.818163
445.054581	8000.363706	11.608064	-0.087735	4.818175
444.784201	8000.317848	11.613069	-0.087685	4.818162
445.087368	8000.357846	11.618074	-0.087741	4.818173
445.104593	8000.297051	11.623079	-0.087745	4.818155
445.028456	8000.323349	11.628083	-0.087730	4.818163
445.611184	8000.251488	11.633088	-0.087839	4.818139
445.106949	8000.252883	11.638093	-0.087745	4.818142
445.048475	8000.367821	11.643098	-0.087734	4.818176
444.958834	8000.315009	11.648103	-0.087717	4.818161
445.103508	8000.323336	11.653107	-0.087744	4.818162
444.872336	8000.332744	11.658112	-0.087701	4.818166
445.107615	8000.292874	11.663117	-0.087745	4.818153
445.518366	8000.269128	11.668122	-0.087822	4.818145
444.737320	8000.300344	11.673127	-0.087676	4.818157
444.760080	8000.304868	11.678131	-0.087680	4.818158
444.603857	8000.427915	11.683136	-0.087651	4.818196
444.346260	8000.442216	11.688141	-0.087603	4.818201
444.649860	8000.388566	11.693146	-0.087660	4.818184
445.102736	8000.290693	11.698151	-0.087744	4.818153
445.129700	8000.336316	11.703155	-0.087749	4.818166
444.797314	8000.326425	11.708160	-0.087687	4.818165
444.540821	8000.339690	11.713165	-0.087639	4.818170
444.963159	8000.328732	11.718170	-0.087718	4.818165
445.446192	8000.237593	11.723175	-0.087808	4.818136
444.759940	8000.311168	11.728179	-0.087680	4.818160
445.491712	8000.261375	11.733184	-0.087816	4.818142
445.340252	8000.296095	11.738189	-0.087788	4.818153
445.369618	8000.314392	11.743194	-0.087794	4.818159
445.141629	8000.282804	11.748199	-0.087751	4.818150
445.127751	8000.305760	11.753203	-0.087749	4.818157
445.020724	8000.385296	11.758208	-0.087729	4.818181
444.849930	8000.345033	11.763213	-0.087697	4.818170
445.029795	8000.388577	11.768218	-0.087730	4.818182
445.384990	8000.294605	11.773223	-0.087796	4.818153
445.217618	8000.279645	11.778227	-0.087765	4.818149
445.378444	8000.298721	11.783232	-0.087795	4.818154
445.651655	8000.229915	11.788237	-0.087846	4.818133
445.758296	8000.280857	11.793242	-0.087866	4.818147
445.483445	8000.254930	11.798247	-0.087815	4.818141
445.402796	8000.298002	11.803251	-0.087800	4.818154
445.418097	8000.307685	11.808256	-0.087802	4.818157
445.287437	8000.267981	11.813261	-0.087778	4.818145
445.136966	8000.319552	11.818266	-0.087750	4.818161
444.916491	8000.281755	11.823271	-0.087709	4.818151
445.071532	8000.307063	11.828275	-0.087738	4.818158
444.903696	8000.364706	11.833280	-0.087707	4.818176
444.902459	8000.354165	11.838285	-0.087706	4.818172
444.595833	8000.439340	11.843290	-0.087649	4.818199
444.715054	8000.324194	11.848295	-0.087671	4.818164
445.047563	8000.319351	11.853299	-0.087733	4.818162
445.061123	8000.362683	11.858304	-0.087736	4.818174
444.746774	8000.348834	11.863309	-0.087677	4.818172
444.931741	8000.327206	11.868314	-0.087712	4.818164
445.008233	8000.309328	11.873319	-0.087726	4.818159
444.636847	8000.378869	11.878323	-0.087657	4.818181
444.733554	8000.333913	11.883328	-0.087675	4.818167
445.169793	8000.273691	11.888333	-0.087756	4.818147
444.706231	8000.406139	11.893338	-0.087670	4.818189
444.635621	8000.350435	11.898343	-0.087656	4.818172
445.192735	8000.261379	11.903347	-0.087760	4.818144
444.924478	8000.312362	11.908352	-0.087710	4.818160
445.149083	8000.268135	11.913357	-0.087752	4.818146
445.021221	8000.327387	11.918362	-0.087728	4.818164
444.875554	8000.368502	11.923367	-0.087701	4.818177
444.879431	8000.393810	11.928371	-0.087702	4.818184
445.090917	8000.325197	11.933376	-0.087741	4.818163
445.882523	8000.201524	11.938381	-0.087888	4.818123
446.139429	8000.225095	11.943386	-0.087936	4.818129
445.133161	8000.277375	11.948391	-0.087749	4.818149
445.408340	8000.289625	11.953395	-0.087800	4.818151
445.319034	8000.321001	11.958400	-0.087783	4.818161
445.288713	8000.281642	11.963405	-0.087778	4.818149
445.389705	8000.299884	11.968410	-0.087797	4.818154
445.481185	8000.266431	11.973415	-0.087814	4.818144
445.119835	8000.312961	11.978419	-0.087746	4.818159
445.527768	8000.286019	11.983424	-0.087822	4.818150
445.968981	8000.241651	11.988429	-0.087904	4.818135
446.308477	8000.231647	11.993434	-0.087968	4.818130
445.723392	8000.263484	11.998439	-0.087859	4.818142
445.987621	8000.260849	12.003443	-0.087908	4.818140
446.195339	8000.265846	12.008448	-0.087946	4.818141
446.022557	8000.209770	12.013453	-0.087914	4.818125
445.973909	8000.241713	12.018458	-0.087905	4.818135
445.805402	8000.266725	12.023463	-0.087874	4.818143
445.742524	8000.277423	12.028467	-0.087862	4.818146
445.793911	8000.246568	12.033472	-0.087872	4.818137
446.013485	8000.247521	12.038477	-0.087912	4.818136
446.025375	8000.228743	12.043482	-0.087915	4.818131
445.562533	8000.260179	12.048487	-0.087828	4.818142
445.827176	8000.289119	12.053491	-0.087878	4.818149
446.044042	8000.315290	12.058496	-0.087918	4.818156
445.578768	8000.293023	12.063501	-0.087831	4.818152
445.511407	8000.312078	12.068506	-0.087819	4.818157
445.923982	8000.246266	12.073511	-0.087896	4.818136
446.004219	8000.266324	12.078515	-0.087911	4.818142
445.845786	8000.287267	12.083520	-0.087881	4.818149
445.914808	8000.262971	12.088525	-0.087894	4.818141
446.089832	8000.267513	12.093530	-0.087927	4.818142
445.488953	8000.275979	12.098535	-0.087815	4.818147
445.770078	8000.266213	12.103539	-0.087867	4.818143
445.983556	8000.272342	12.108544	-0.087907	4.818144
445.701707	8000.254735	12.113549	-0.087854	4.818140
445.715662	8000.289655	12.118554	-0.087857	4.818150
446.124810	8000.244841	12.123559	-0.087933	4.818135
446.201519	8000.210130	12.128563	-0.087947	4.818124
446.450039	8000.189387	12.133568	-0.087993	4.818117
446.277376	8000.174353	12.138573	-0.087961	4.818113
445.956574	8000.282481	12.143578	-0.087902	4.818147
445.951339	8000.246628	12.148583	-0.087901	4.818136
446.464825	8000.182222	12.153587	-0.087996	4.818115
446.285474	8000.251280	12.158592	-0.087963	4.818136
446.517844	8000.189272	12.163597	-0.088006	4.818117
446.613545	8000.222174	12.168602	-0.088024	4.818126
446.322961	8000.200235	12.173607	-0.087970	4.818121
446.440513	8000.217656	12.178611	-0.087992	4.818126
446.099656	8000.247633	12.183616	-0.087928	4.818136
446.552438	8000.161335	12.188621	-0.088012	4.818108
446.665757	8000.160807	12.193626	-0.088033	4.818108
446.781165	8000.102431	12.198631	-0.088055	4.818090
446.922270	8000.082297	12.203635	-0.088081	4.818083
446.458052	8000.192637	12.208640	-0.087995	4.818118
446.297152	8000.199865	12.213645	-0.087965	4.818121
446.589314	8000.210248	12.218650	-0.088019	4.818123
446.526344	8000.172538	12.223655	-0.088007	4.818112
446.408648	8000.201415	12.228659	-0.087985	4.818121
446.060509	8000.260756	12.233664	-0.087921	4.818140
446.212675	8000.209206	12.238669	-0.087949	4.818124
446.100464	8000.272886	12.243674	-0.087928	4.818143
446.235750	8000.193740	12.248679	-0.087953	4.818119
446.117573	8000.195250	12.253683	-0.087931	4.818120
446.372753	8000.203012	12.258688	-0.087979	4.818122
446.662309	8000.164952	12.263693	-0.088033	4.818109
446.318908	8000.232777	12.268698	-0.087969	4.818131
446.383906	8000.190536	12.273703	-0.087981	4.818118
445.974669	8000.251131	12.278707	-0.087904	4.818137
446.064044	8000.250270	12.283712	-0.087921	4.818137
446.229788	8000.211537	12.288717	-0.087952	4.818125
446.513566	8000.252320	12.293722	-0.088005	4.818136
446.409561	8000.171945	12.298727	-0.087985	4.818112
446.278159	8000.179585	12.303731	-0.087961	4.818115
446.345602	8000.232087	12.308736	-0.087973	4.818130
446.554129	8000.185531	12.313741	-0.088012	4.818116
446.017738	8000.227517	12.318746	-0.087912	4.818130
445.721725	8000.244440	12.323751	-0.087857	4.818137
446.325993	8000.201291	12.328755	-0.087970	4.818121
445.882096	8000.239305	12.333760	-0.087887	4.818134
446.050602	8000.204819	12.338765	-0.087918	4.818123
446.145215	8000.249281	12.343770	-0.087936	4.818136
446.113817	8000.233058	12.348775	-0.087930	4.818132
445.925275	8000.233587	12.353779	-0.087895	4.818133
446.520629	8000.207152	12.358784	-0.088006	4.818122
446.377191	8000.210415	12.363789	-0.087979	4.818124
446.219813	8000.289250	12.368794	-0.087950	4.818148
446.187582	8000.241445	12.373799	-0.087944	4.818134
446.176237	8000.244443	12.378803	-0.087942	4.818135
446.324980	8000.227572	12.383808	-0.087969	4.818129
446.203371	8000.221667	12.388813	-0.087947	4.818128
446.152410	8000.240950	12.393818	-0.087937	4.818134
445.903879	8000.224860	12.398823	-0.087891	4.818130
445.802108	8000.269743	12.403827	-0.087872	4.818144
445.866242	8000.294838	12.408832	-0.087884	4.818151
446.170807	8000.234888	12.413837	-0.087941	4.818132
446.221636	8000.198763	12.418842	-0.087950	4.818121
445.927084	8000.172561	12.423847	-0.087895	4.818114
445.655293	8000.260326	12.428851	-0.087845	4.818142
446.474886	8000.224386	12.433856	-0.087997	4.818128
446.211082	8000.200716	12.438861	-0.087948	4.818122
446.427174	8000.238452	12.443866	-0.087988	4.818132
446.288396	8000.197581	12.448871	-0.087962	4.818120
446.368632	8000.262890	12.453875	-0.087977	4.818139
446.370003	8000.255541	12.458880	-0.087977	4.818137
445.848327	8000.299837	12.463885	-0.087880	4.818152
446.312542	8000.270523	12.468890	-0.087967	4.818142
445.845296	8000.242967	12.473895	-0.087880	4.818136
445.396721	8000.299857	12.478899	-0.087796	4.818154
445.908427	8000.250158	12.483904	-0.087891	4.818137
446.318472	8000.173787	12.488909	-0.087968	4.818113
446.243388	8000.228513	12.493914	-0.087954	4.818130
446.215280	8000.215492	12.498919	-0.087949	4.818126
446.137781	8000.241772	12.503923	-0.087934	4.818134
445.715691	8000.291665	12.508928	-0.087856	4.818151
445.962647	8000.254063	12.513933	-0.087901	4.818138
446.116573	8000.298298	12.518938	-0.087930	4.818151
446.128484	8000.243742	12.523943	-0.087932	4.818135
445.930419	8000.330430	12.528947	-0.087895	4.818161
445.831062	8000.314312	12.533952	-0.087877	4.818157
445.617129	8000.278709	12.538957	-0.087837	4.818147
445.358269	8000.324561	12.543962	-0.087789	4.818162
445.344303	8000.312790	12.548967	-0.087786	4.818158
445.985415	8000.266998	12.553971	-0.087906	4.818142
445.494910	8000.312781	12.558976	-0.087814	4.818158
445.553636	8000.280976	12.563981	-0.087825	4.818148
445.677223	8000.325841	12.568986	-0.087848	4.818161
445.806425	8000.263448	12.573991	-0.087872	4.818142
445.868862	8000.264316	12.578995	-0.087884	4.818142
445.417057	8000.375881	12.584000	-0.087800	4.818177
445.372012	8000.321585	12.589005	-0.087791	4.818161
445.939955	8000.267407	12.594010	-0.087897	4.818142
445.534343	8000.310163	12.599015	-0.087821	4.818157
445.782897	8000.294682	12.604019	-0.087868	4.818151
446.075487	8000.302966	12.609024	-0.087922	4.818152
446.098389	8000.251720	12.614029	-0.087926	4.818137
445.391062	8000.433388	12.619034	-0.087795	4.818194
445.371201	8000.339454	12.624039	-0.087791	4.818166
445.659918	8000.286649	12.629043	-0.087845	4.818149
445.207576	8000.431881	12.634048	-0.087761	4.818194
445.304858	8000.297487	12.639053	-0.087779	4.818154
445.783913	8000.279954	12.644058	-0.087868	4.818147
445.912731	8000.252282	12.649063	-0.087892	4.818138
445.930880	8000.256743	12.654067	-0.087895	4.818139
445.955691	8000.259192	12.659072	-0.087900	4.818140
445.831340	8000.273243	12.664077	-0.087877	4.818145
445.721301	8000.300122	12.669082	-0.087856	4.818153
446.030421	8000.256020	12.674087	-0.087914	4.818139
445.649318	8000.302274	12.679091	-0.087843	4.818154
445.972878	8000.279419	12.684096	-0.087903	4.818146
446.221492	8000.247102	12.689101	-0.087949	4.818135
446.189084	8000.249807	12.694106	-0.087943	4.818136
445.970264	8000.218345	12.699111	-0.087902	4.818128
445.861446	8000.255764	12.704115	-0.087882	4.818139
446.264186	8000.260320	12.709120	-0.087957	4.818139
446.257906	8000.223400	12.714125	-0.087956	4.818128
446.320367	8000.262153	12.719130	-0.087967	4.818139
445.922781	8000.272398	12.724135	-0.087893	4.818144
446.120618	8000.270943	12.729139	-0.087930	4.818143
446.015019	8000.316825	12.734144	-0.087911	4.818157
446.335831	8000.210799	12.739149	-0.087970	4.818124
446.267046	8000.262456	12.744154	-0.087957	4.818140
446.592016	8000.225941	12.749159	-0.088018	4.818128
446.790031	8000.173977	12.754163	-0.088055	4.818111
446.830753	8000.226108	12.759168	-0.088062	4.818127
446.035994	8000.252919	12.764173	-0.087914	4.818138
446.565468	8000.246613	12.769178	-0.088013	4.818134
446.381853	8000.216693	12.774183	-0.087979	4.818126
445.955022	8000.273886	12.779187	-0.087899	4.818144
446.362581	8000.249044	12.784192	-0.087975	4.818135
446.440747	8000.186993	12.789197	-0.087990	4.818117
446.234887	8000.225164	12.794202	-0.087951	4.818129
446.673549	8000.191286	12.799207	-0.088033	4.818117
446.368271	8000.220706	12.804211	-0.087976	4.818127
446.391872	8000.209458	12.809216	-0.087980	4.818123
446.332305	8000.217046	12.814221	-0.087969	4.818126
446.430384	8000.259451	12.819226	-0.087988	4.818138
446.434587	8000.236358	12.824231	-0.087988	4.818131
446.247885	8000.220075	12.829235	-0.087954	4.818127
446.412676	8000.259201	12.834240	-0.087984	4.818138
446.520670	8000.208088	12.839245	-0.088004	4.818123
446.346135	8000.248801	12.844250	-0.087972	4.818135
446.483320	8000.195990	12.849255	-0.087997	4.818119
446.427055	8000.218356	12.854259	-0.087987	4.818126
446.329504	8000.240147	12.859264	-0.087969	4.818133
446.459524	8000.213544	12.864269	-0.087993	4.818124
446.842740	8000.212568	12.869274	-0.088064	4.818123
446.061636	8000.215365	12.874279	-0.087919	4.818127
446.336536	8000.172891	12.879283	-0.087970	4.818113
446.358453	8000.238439	12.884288	-0.087974	4.818132
446.485415	8000.202323	12.889293	-0.087998	4.818121
446.379960	8000.236632	12.894298	-0.087978	4.818132
445.775995	8000.273467	12.899303	-0.087865	4.818145
446.294873	8000.255438	12.904307	-0.087962	4.818137
446.111838	8000.284457	12.909312	-0.087928	4.818147
446.420188	8000.250868	12.914317	-0.087985	4.818136
446.302648	8000.265014	12.919322	-0.087963	4.818140
446.268665	8000.268748	12.924327	-0.087957	4.818142
446.344563	8000.270857	12.929331	-0.087971	4.818142
446.400214	8000.249532	12.934336	-0.087982	4.818135
446.028498	8000.248562	12.939341	-0.087912	4.818137
446.125622	8000.279379	12.944346	-0.087930	4.818145
446.389871	8000.255698	12.949351	-0.087980	4.818137
446.516849	8000.230105	12.954355	-0.088003	4.818129
446.272801	8000.265640	12.959360	-0.087958	4.818141
445.955733	8000.280164	12.964365	-0.087899	4.818146
446.197441	8000.304577	12.969370	-0.087944	4.818152
446.066372	8000.306959	12.974375	-0.087919	4.818154
446.427363	8000.263580	12.979379	-0.087986	4.818139
446.295128	8000.299620	12.984384	-0.087962	4.818151
446.205818	8000.272066	12.989389	-0.087945	4.818143
446.448404	8000.270183	12.994394	-0.087990	4.818141
446.447996	8000.232292	12.999399	-0.087990	4.818130
446.386968	8000.268272	13.004403	-0.087979	4.818141
446.521260	8000.278561	13.009408	-0.088004	4.818143
446.715866	8000.227602	13.014413	-0.088040	4.818128
446.770122	8000.245194	13.019418	-0.088050	4.818133
446.851176	8000.211595	13.024423	-0.088065	4.818122
446.551968	8000.243204	13.029427	-0.088010	4.818133
446.239701	8000.308306	13.034432	-0.087951	4.818153
446.501115	8000.226708	13.039437	-0.088000	4.818128
446.256192	8000.287487	13.044442	-0.087954	4.818147
446.316517	8000.263071	13.049447	-0.087966	4.818140
446.310001	8000.293496	13.054451	-0.087964	4.818149
446.863354	8000.261216	13.059456	-0.088067	4.818137
447.021149	8000.218163	13.064461	-0.088097	4.818123
446.873936	8000.251890	13.069466	-0.088069	4.818134
446.421284	8000.261367	13.074471	-0.087985	4.818139
446.383689	8000.263999	13.079475	-0.087978	4.818140
446.377285	8000.277589	13.084480	-0.087977	4.818144
446.801933	8000.220364	13.089485	-0.088056	4.818125
446.870472	8000.244469	13.094490	-0.088069	4.818132
446.946424	8000.216061	13.099495	-0.088083	4.818123
446.779833	8000.247413	13.104499	-0.088052	4.818133
446.622773	8000.250485	13.109504	-0.088022	4.818135
446.539969	8000.235650	13.114509	-0.088007	4.818131
446.568785	8000.261306	13.119514	-0.088012	4.818138
446.879453	8000.254058	13.124519	-0.088070	4.818135
446.921400	8000.195710	13.129523	-0.088078	4.818117
446.860843	8000.216965	13.134528	-0.088067	4.818124
446.828757	8000.202836	13.139533	-0.088061	4.818120
446.791494	8000.185478	13.144538	-0.088054	4.818115
446.286308	8000.248945	13.149543	-0.087960	4.818136
446.273198	8000.277174	13.154547	-0.087957	4.818144
446.729319	8000.269847	13.159552	-0.088042	4.818140
446.477268	8000.256863	13.164557	-0.087995	4.818137
446.272268	8000.288733	13.169562	-0.087957	4.818147
446.801709	8000.231916	13.174567	-0.088056	4.818128
446.196075	8000.281355	13.179571	-0.087943	4.818146
446.014762	8000.327235	13.184576	-0.087909	4.818160
446.326490	8000.256861	13.189581	-0.087967	4.818138
445.847227	8000.369096	13.194586	-0.087878	4.818173
446.045034	8000.346595	13.199591	-0.087915	4.818166
446.094510	8000.277829	13.204595	-0.087924	4.818145
445.758456	8000.402583	13.209600	-0.087861	4.818183
445.633236	8000.335593	13.214605	-0.087838	4.818164
446.037145	8000.290707	13.219610	-0.087913	4.818149
445.679836	8000.395170	13.224615	-0.087847	4.818182
445.609484	8000.340520	13.229619	-0.087833	4.818166
445.773213	8000.338590	13.234624	-0.087864	4.818164
446.295775	8000.331136	13.239629	-0.087961	4.818160
446.829344	8000.292267	13.244634	-0.088060	4.818146
446.462230	8000.263999	13.249639	-0.087992	4.818139
446.645974	8000.262349	13.254643	-0.088026	4.818138
446.246275	8000.307291	13.259648	-0.087952	4.818153
445.864925	8000.349332	13.264653	-0.087881	4.818167
445.880402	8000.353755	13.269658	-0.087884	4.818168
445.577706	8000.379002	13.274663	-0.087827	4.818177
445.810051	8000.339093	13.279667	-0.087871	4.818164
446.154419	8000.329156	13.284672	-0.087935	4.818160
445.916283	8000.262698	13.289677	-0.087890	4.818141
446.381825	8000.273391	13.294682	-0.087977	4.818142
445.962473	8000.289647	13.299687	-0.087899	4.818149
446.127737	8000.298262	13.304691	-0.087930	4.818151
446.681177	8000.285977	13.309696	-0.088033	4.818145
446.409262	8000.244304	13.314701	-0.087982	4.818134
446.581791	8000.258282	13.319706	-0.088014	4.818137
447.258862	8000.178266	13.324711	-0.088140	4.818111
446.959009	8000.184610	13.329715	-0.088084	4.818114
446.413459	8000.283293	13.334720	-0.087983	4.818145
446.501175	8000.262415	13.339725	-0.087999	4.818139
446.810720	8000.246733	13.344730	-0.088057	4.818133
446.783599	8000.221097	13.349735	-0.088052	4.818125
446.520841	8000.227959	13.354739	-0.088003	4.818128
447.055352	8000.234353	13.359744	-0.088102	4.818128
446.557455	8000.266350	13.364749	-0.088009	4.818140
446.920171	8000.224048	13.369754	-0.088077	4.818126
446.552109	8000.242070	13.374759	-0.088008	4.818133
446.811087	8000.242520	13.379763	-0.088057	4.818132
446.313928	8000.288208	13.384768	-0.087964	4.818147
446.148959	8000.290118	13.389773	-0.087933	4.818148
445.983612	8000.340430	13.394778	-0.087903	4.818164
446.276092	8000.260317	13.399783	-0.087957	4.818139
445.860341	8000.355547	13.404787	-0.087880	4.818169
445.531068	8000.488813	13.409792	-0.087818	4.818210
445.537579	8000.435234	13.414797	-0.087819	4.818194
445.562274	8000.395589	13.419802	-0.087824	4.818182
445.765007	8000.387889	13.424807	-0.087862	4.818179
446.095450	8000.314619	13.429811	-0.087923	4.818156
446.224082	8000.295363	13.434816	-0.087947	4.818150
446.093497	8000.324060	13.439821	-0.087923	4.818159
446.461115	8000.348123	13.444826	-0.087991	4.818164
446.284578	8000.331981	13.449831	-0.087958	4.818160
446.246022	8000.279879	13.454835	-0.087951	4.818145
446.813563	8000.250953	13.459840	-0.088057	4.818134
446.217054	8000.253165	13.464845	-0.087946	4.818137
446.249278	8000.308333	13.469850	-0.087952	4.818153
446.075080	8000.372202	13.474855	-0.087919	4.818173
446.246233	8000.270405	13.479859	-0.087951	4.818142
445.881012	8000.360025	13.484864	-0.087883	4.818170
445.939824	8000.333483	13.489869	-0.087894	4.818162
446.632128	8000.287353	13.494874	-0.088023	4.818146
446.507366	8000.299294	13.499879	-0.088000	4.818150
446.134224	8000.286728	13.504883	-0.087930	4.818147
446.083968	8000.358637	13.509888	-0.087921	4.818169
446.129058	8000.345584	13.514893	-0.087929	4.818165
445.993854	8000.421571	13.519898	-0.087904	4.818188
446.174438	8000.334638	13.524903	-0.087938	4.818162
446.049963	8000.339217	13.529907	-0.087914	4.818163
445.966220	8000.398031	13.534912	-0.087899	4.818181
445.870270	8000.351443	13.539917	-0.087881	4.818168
446.086096	8000.375495	13.544922	-0.087921	4.818174
446.036830	8000.404273	13.549927	-0.087912	4.818183
446.157424	8000.331237	13.554931	-0.087934	4.818161
446.347594	8000.334937	13.559936	-0.087970	4.818161
445.929518	8000.345949	13.564941	-0.087892	4.818166
445.973918	8000.380240	13.569946	-0.087900	4.818176
446.235724	8000.365997	13.574951	-0.087949	4.818171
446.419367	8000.363293	13.579955	-0.087983	4.818169
446.743489	8000.344657	13.584960	-0.088043	4.818162
446.121045	8000.331773	13.589965	-0.087927	4.818161
446.689852	8000.284976	13.594970	-0.088033	4.818145
446.466779	8000.286076	13.599975	-0.087992	4.818146
446.293509	8000.279451	13.604979	-0.087960	4.818145
446.572053	8000.273860	13.609984	-0.088011	4.818142
446.914749	8000.217598	13.614989	-0.088075	4.818124
446.832158	8000.261697	13.619994	-0.088060	4.818137
446.498047	8000.265459	13.624999	-0.087998	4.818140
446.128100	8000.312920	13.630003	-0.087929	4.818155
446.421040	8000.295954	13.635008	-0.087983	4.818149
446.623021	8000.233522	13.640013	-0.088021	4.818130
446.744774	8000.263630	13.645018	-0.088043	4.818138
446.776931	8000.277757	13.650023	-0.088049	4.818142
446.973879	8000.216308	13.655027	-0.088086	4.818123
446.608350	8000.289086	13.660032	-0.088018	4.818146
446.477426	8000.279894	13.665037	-0.087994	4.818144
446.144431	8000.308929	13.670042	-0.087932	4.818154
446.254349	8000.322034	13.675047	-0.087952	4.818157
446.647041	8000.263312	13.680051	-0.088025	4.818138
446.876406	8000.281240	13.685056	-0.088068	4.818143
446.518230	8000.274143	13.690061	-0.088001	4.818142
446.238429	8000.344959	13.695066	-0.087949	4.818164
446.903834	8000.244786	13.700071	-0.088073	4.818132
446.380771	8000.265910	13.705075	-0.087975	4.818140
446.546755	8000.278745	13.710080	-0.088006	4.818143
446.688416	8000.234415	13.715085	-0.088033	4.818130
446.533536	8000.273296	13.720090	-0.088004	4.818142
446.668737	8000.278336	13.725095	-0.088029	4.818143
446.858779	8000.273617	13.730099	-0.088064	4.818141
446.815726	8000.308795	13.735104	-0.088056	4.818151
446.466172	8000.293400	13.740109	-0.087991	4.818148
446.264249	8000.314789	13.745114	-0.087954	4.818155
446.949605	8000.232784	13.750119	-0.088081	4.818128
447.165373	8000.228423	13.755123	-0.088121	4.818126
447.208986	8000.247972	13.760128	-0.088129	4.818132
446.945656	8000.253772	13.765133	-0.088080	4.818134
447.055184	8000.258454	13.770138	-0.088101	4.818135
446.516353	8000.323556	13.775143	-0.088000	4.818157
446.489085	8000.280029	13.780147	-0.087995	4.818144
446.698527	8000.316621	13.785152	-0.088034	4.818154
446.508965	8000.279251	13.790157	-0.087999	4.818144
446.566980	8000.315837	13.795162	-0.088010	4.818154
446.759373	8000.253272	13.800167	-0.088046	4.818135
446.573646	8000.272782	13.805171	-0.088011	4.818142
446.567465	8000.327416	13.810176	-0.088010	4.818158
446.564007	8000.307372	13.815181	-0.088009	4.818152
446.594303	8000.359358	13.820186	-0.088015	4.818167
446.512033	8000.326640	13.825191	-0.088000	4.818158
446.579921	8000.297067	13.830195	-0.088012	4.818149
446.949816	8000.269598	13.835200	-0.088081	4.818139
446.421397	8000.324321	13.840205	-0.087983	4.818157
446.188196	8000.329490	13.845210	-0.087939	4.818160
446.508143	8000.336051	13.850215	-0.087999	4.818161
446.568892	8000.280070	13.855219	-0.088010	4.818144
446.064555	8000.385641	13.860224	-0.087916	4.818177
446.525016	8000.276299	13.865229	-0.088002	4.818143
446.560707	8000.313627	13.870234	-0.088008	4.818154
446.169896	8000.349222	13.875239	-0.087936	4.818166
446.422347	8000.268551	13.880243	-0.087983	4.818141
446.549582	8000.303997	13.885248	-0.088006	4.818151
446.491018	8000.294761	13.890253	-0.087995	4.818148
446.699682	8000.283987	13.895258	-0.088034	4.818144
446.692089	8000.262834	13.900263	-0.088033	4.818138
446.591859	8000.301425	13.905267	-0.088014	4.818150
446.260935	8000.412569	13.910272	-0.087953	4.818184
446.215599	8000.306703	13.915277	-0.087944	4.818153
446.733272	8000.303391	13.920282	-0.088040	4.818150
446.825602	8000.266792	13.925287	-0.088058	4.818139
446.990615	8000.272248	13.930291	-0.088088	4.818140
446.789120	8000.335736	13.935296	-0.088051	4.818159
446.622029	8000.330249	13.940301	-0.088020	4.818158
446.056190	8000.387609	13.945306	-0.087914	4.818178
446.417525	8000.290566	13.950311	-0.087981	4.818147
446.793678	8000.271602	13.955315	-0.088052	4.818140
446.350276	8000.392755	13.960320	-0.087969	4.818178
445.870735	8000.419747	13.965325	-0.087880	4.818188
446.534877	8000.365860	13.970330	-0.088003	4.818169
446.835612	8000.277443	13.975335	-0.088059	4.818142
446.675286	8000.315197	13.980339	-0.088029	4.818154
446.374938	8000.373098	13.985344	-0.087974	4.818172
446.461041	8000.289058	13.990349	-0.087989	4.818147
446.380426	8000.337393	13.995354	-0.087974	4.818162
446.670614	8000.298289	14.000359	-0.088028	4.818149
446.472224	8000.342879	14.005363	-0.087992	4.818163
447.037998	8000.309721	14.010368	-0.088097	4.818151
446.709773	8000.308302	14.015373	-0.088036	4.818152
446.763070	8000.300625	14.020378	-0.088046	4.818149
446.750099	8000.334118	14.025383	-0.088043	4.818159
446.690467	8000.300663	14.030387	-0.088032	4.818149
446.340372	8000.379971	14.035392	-0.087967	4.818174
446.574152	8000.304302	14.040397	-0.088010	4.818151
446.483797	8000.320931	14.045402	-0.087994	4.818156
446.386064	8000.364819	14.050407	-0.087975	4.818170
446.981759	8000.285774	14.055411	-0.088086	4.818144
446.843339	8000.277530	14.060416	-0.088060	4.818142
445.874604	8000.399782	14.065421	-0.087880	4.818182
445.971503	8000.374823	14.070426	-0.087898	4.818174
446.547094	8000.291288	14.075431	-0.088005	4.818147
446.877213	8000.250636	14.080435	-0.088067	4.818134
446.825471	8000.298322	14.085440	-0.088057	4.818148
447.071522	8000.219667	14.090445	-0.088103	4.818124
446.954823	8000.278023	14.095450	-0.088081	4.818142
446.671127	8000.294063	14.100455	-0.088028	4.818147
447.392905	8000.225194	14.105459	-0.088163	4.818124
447.221612	8000.282790	14.110464	-0.088131	4.818142
446.595677	8000.294060	14.115469	-0.088014	4.818148
446.682370	8000.325785	14.120474	-0.088030	4.818157
446.615948	8000.331172	14.125479	-0.088018	4.818159
446.291034	8000.371894	14.130483	-0.087957	4.818172
446.582141	8000.369635	14.135488	-0.088012	4.818170
446.786956	8000.260940	14.140493	-0.088050	4.818137
447.058610	8000.262619	14.145498	-0.088100	4.818137
446.957031	8000.267517	14.150503	-0.088081	4.818138
447.393807	8000.248346	14.155507	-0.088163	4.818131
447.768479	8000.248306	14.160512	-0.088232	4.818129
447.365412	8000.237425	14.165517	-0.088157	4.818128
447.233659	8000.255582	14.170522	-0.088133	4.818134
447.093155	8000.258884	14.175527	-0.088107	4.818135
446.754618	8000.284683	14.180531	-0.088044	4.818144
446.795088	8000.318921	14.185536	-0.088051	4.818154
446.872405	8000.260013	14.190541	-0.088065	4.818137
446.599777	8000.302516	14.195546	-0.088015	4.818150
446.804884	8000.260122	14.200551	-0.088053	4.818137
446.669318	8000.289802	14.205555	-0.088028	4.818146
447.010263	8000.299814	14.210560	-0.088091	4.818148
446.810758	8000.273881	14.215565	-0.088054	4.818141
446.784447	8000.271409	14.220570	-0.088049	4.818140
447.318692	8000.278853	14.225575	-0.088148	4.818140
447.044680	8000.267666	14.230579	-0.088097	4.818138
447.159230	8000.274523	14.235584	-0.088119	4.818140
447.012776	8000.286161	14.240589	-0.088091	4.818144
447.305055	8000.293391	14.245594	-0.088146	4.818145
447.383081	8000.256592	14.250599	-0.088160	4.818133
447.334338	8000.270645	14.255603	-0.088151	4.818138
447.492556	8000.286529	14.260608	-0.088181	4.818142
447.030819	8000.271674	14.265613	-0.088095	4.818139
447.148739	8000.243850	14.270618	-0.088117	4.818131
447.021711	8000.289434	14.275623	-0.088093	4.818145
447.046472	8000.276098	14.280627	-0.088098	4.818141
447.151815	8000.278617	14.285632	-0.088117	4.818141
447.215421	8000.230042	14.290637	-0.088129	4.818126
446.820545	8000.319249	14.295642	-0.088055	4.818154
446.652788	8000.324276	14.300647	-0.088024	4.818157
446.898357	8000.248771	14.305651	-0.088070	4.818133
447.119696	8000.299210	14.310656	-0.088111	4.818147
447.351290	8000.219301	14.315661	-0.088154	4.818123
446.779595	8000.302887	14.320666	-0.088048	4.818150
446.643724	8000.359923	14.325671	-0.088022	4.818167
446.607395	8000.315217	14.330675	-0.088016	4.818154
446.769038	8000.355353	14.335680	-0.088046	4.818165
447.029472	8000.284265	14.340685	-0.088094	4.818143
447.040175	8000.305460	14.345690	-0.088096	4.818149
447.047855	8000.291885	14.350695	-0.088098	4.818145
447.361989	8000.222597	14.355699	-0.088156	4.818123
447.445177	8000.282687	14.360704	-0.088172	4.818141
447.251683	8000.261047	14.365709	-0.088135	4.818135
447.212928	8000.265767	14.370714	-0.088128	4.818137
446.542419	8000.377441	14.375719	-0.088003	4.818173
446.460438	8000.352094	14.380723	-0.087988	4.818166
447.060821	8000.325732	14.385728	-0.088100	4.818155
446.994003	8000.279549	14.390733	-0.088087	4.818142
447.485233	8000.286394	14.395738	-0.088179	4.818142
447.305201	8000.280727	14.400743	-0.088145	4.818141
447.270523	8000.243410	14.405747	-0.088139	4.818130
447.074967	7999.298862	14.410752	-0.088102	4.817851

447.429647	7996.148279	14.415757	-0.088166	4.816914
447.106700	7990.671820	14.420762	-0.088102	4.815290
446.902259	7984.091858	14.425767	-0.088060	4.813337
447.008301	7976.753781	14.430771	-0.088075	4.811157
446.468225	7969.225624	14.435776	-0.087969	4.808922
446.506363	7961.377993	14.440781	-0.087971	4.806589
446.698774	7953.406030	14.445786	-0.088002	4.804217
446.639036	7945.573200	14.450791	-0.087985	4.801886
446.607631	7937.534904	14.455795	-0.087974	4.799493
446.432389	7929.618322	14.460800	-0.087937	4.797135
446.598156	7921.519215	14.465805	-0.087962	4.794720
446.309725	7913.606117	14.470810	-0.087903	4.792362
446.409128	7905.560314	14.475815	-0.087916	4.789961
446.199883	7897.568311	14.480819	-0.087872	4.787576
446.018159	7889.543065	14.485824	-0.087833	4.785180
446.227320	7881.515792	14.490829	-0.087867	4.782781
446.692900	7873.521363	14.495834	-0.087948	4.780389
446.530555	7865.573112	14.500839	-0.087913	4.778012
446.044038	7857.562911	14.505843	-0.087817	4.775617
446.393492	7849.527988	14.510848	-0.087877	4.773210
446.300920	7841.510248	14.515853	-0.087854	4.770809
446.461103	7833.479302	14.520858	-0.087879	4.768401
446.423864	7825.535799	14.525863	-0.087867	4.766019
445.832047	7817.535879	14.530867	-0.087751	4.763621
446.147807	7809.546592	14.535872	-0.087805	4.761222
446.160831	7801.449330	14.540877	-0.087802	4.758790
446.288745	7793.566035	14.545882	-0.087821	4.756421
445.931165	7785.544298	14.550887	-0.087749	4.754011
446.160001	7777.554610	14.555891	-0.087786	4.751607
445.755644	7769.543898	14.560896	-0.087706	4.749198
445.969623	7761.487507	14.565901	-0.087740	4.746772
445.411724	7753.467365	14.570906	-0.087631	4.744357
445.560143	7745.519142	14.575911	-0.087654	4.741961
445.311776	7737.492185	14.580915	-0.087602	4.739541
445.413047	7729.541323	14.585920	-0.087616	4.737142
445.129308	7721.410743	14.590925	-0.087558	4.734689
445.014647	7713.551282	14.595930	-0.087531	4.732316
445.547832	7705.448164	14.600935	-0.087625	4.729866
445.347466	7697.449524	14.605939	-0.087583	4.727448
444.944905	7689.509492	14.610944	-0.087503	4.725047
445.075895	7681.510958	14.615949	-0.087522	4.722627
445.162749	7673.457459	14.620954	-0.087533	4.720188
445.059580	7665.518268	14.625959	-0.087508	4.717783
445.136617	7657.455462	14.630963	-0.087517	4.715339
444.967273	7649.575598	14.635968	-0.087481	4.712950
444.907953	7641.488461	14.640973	-0.087464	4.710496
445.341065	7633.384400	14.645978	-0.087540	4.708036
445.593812	7625.389394	14.650983	-0.087582	4.705607
445.053607	7617.478964	14.655987	-0.087476	4.703204
444.896611	7609.559102	14.660992	-0.087441	4.700796
444.539723	7601.549142	14.665997	-0.087370	4.698360
444.622709	7593.492970	14.671002	-0.087380	4.695908
444.483367	7585.499571	14.676007	-0.087349	4.693474
444.635525	7577.456132	14.681011	-0.087372	4.691024
445.013012	7569.465756	14.686016	-0.087437	4.688587
444.295524	7561.502401	14.691021	-0.087298	4.686160
444.391983	7553.429375	14.696026	-0.087311	4.683696
444.332281	7545.556396	14.701031	-0.087294	4.681292
444.453985	7537.426409	14.706035	-0.087312	4.678809
444.658271	7529.534771	14.711040	-0.087345	4.676397
444.436446	7521.454252	14.716045	-0.087298	4.673926
444.693758	7513.397481	14.721050	-0.087341	4.671461
444.754361	7505.389356	14.726055	-0.087347	4.669009
444.408638	7497.392870	14.731059	-0.087277	4.666561
444.549089	7489.415732	14.736064	-0.087298	4.664116
444.364956	7481.464690	14.741069	-0.087259	4.661678
444.568984	7473.452198	14.746074	-0.087291	4.659220
444.490534	7465.486304	14.751079	-0.087272	4.656776
443.792799	7457.478420	14.756083	-0.087136	4.654317
443.992565	7449.485718	14.761088	-0.087168	4.651861
444.318387	7441.361163	14.766093	-0.087224	4.649363
444.594653	7433.398137	14.771098	-0.087270	4.646914
444.302924	7425.394589	14.776103	-0.087210	4.644451
444.105095	7417.419719	14.781107	-0.087168	4.641996
444.145238	7409.478440	14.786112	-0.087171	4.639549
443.988660	7401.498928	14.791117	-0.087136	4.637090
443.671456	7393.408469	14.796122	-0.087072	4.634595
443.917456	7385.425122	14.801127	-0.087112	4.632131
443.792566	7377.359426	14.806131	-0.087084	4.629641
443.936703	7369.422043	14.811136	-0.087106	4.627190
444.146641	7361.352378	14.816141	-0.087139	4.624696
443.974277	7353.452191	14.821146	-0.087102	4.622253
443.930737	7345.392574	14.826151	-0.087089	4.619759
443.748105	7337.476776	14.831155	-0.087050	4.617309
443.688618	7329.392647	14.836160	-0.087033	4.614805
443.896440	7321.388807	14.841165	-0.087067	4.612325
443.971339	7313.323123	14.846170	-0.087075	4.609824
443.740189	7305.436745	14.851175	-0.087027	4.607377
443.459134	7297.347664	14.856179	-0.086970	4.604866
443.570228	7289.419602	14.861184	-0.086985	4.602404
443.537211	7281.362657	14.866189	-0.086974	4.599901
443.812780	7273.404352	14.871194	-0.087020	4.597427
443.608312	7265.379856	14.876199	-0.086976	4.594931
443.325848	7257.364139	14.881203	-0.086919	4.592435
443.526294	7249.356844	14.886208	-0.086951	4.589942
443.291637	7241.334740	14.891213	-0.086902	4.587442
443.423437	7233.299378	14.896218	-0.086921	4.584938
443.669412	7225.337856	14.901223	-0.086962	4.582455
443.266073	7217.320837	14.906227	-0.086881	4.579952
442.906071	7209.437081	14.911232	-0.086809	4.577490
442.726061	7201.415875	14.916237	-0.086770	4.574983
442.865997	7193.376372	14.921242	-0.086791	4.572471
442.828558	7185.325312	14.926247	-0.086779	4.569952
442.821257	7177.286511	14.931251	-0.086772	4.567437
442.748342	7169.311370	14.936256	-0.086754	4.564939
442.764865	7161.352010	14.941261	-0.086751	4.562446
442.807652	7153.358993	14.946266	-0.086754	4.559940
442.353401	7145.426487	14.951271	-0.086664	4.557452
442.489885	7137.295444	14.956275	-0.086684	4.554900
442.570890	7129.356192	14.961280	-0.086694	4.552408
441.780570	7121.348223	14.966285	-0.086542	4.549890
442.233237	7113.300824	14.971290	-0.086621	4.547362
442.482912	7105.240456	14.976295	-0.086662	4.544827
441.800765	7097.359544	14.981299	-0.086530	4.542345
442.597888	7089.252060	14.986304	-0.086673	4.539795
442.023272	7081.352497	14.991309	-0.086561	4.537305
442.085747	7073.303527	14.996314	-0.086567	4.534768
442.539314	7065.298179	15.001319	-0.086647	4.532244
441.875998	7057.336777	15.006323	-0.086518	4.529730
441.914100	7049.379587	15.011328	-0.086520	4.527218
441.481112	7041.330431	15.016333	-0.086434	4.524674
440.845023	7033.404431	15.021338	-0.086310	4.522166
441.044303	7025.311147	15.026343	-0.086342	4.519607
440.961164	7017.308025	15.031347	-0.086321	4.517074
441.107037	7009.263746	15.036352	-0.086343	4.514528
440.649436	7001.345440	15.041357	-0.086253	4.512018
440.831206	6993.239908	15.046362	-0.086281	4.509449
441.088588	6985.207991	15.051367	-0.086324	4.506902
440.650431	6977.228417	15.056371	-0.086237	4.504368
440.890118	6969.282370	15.061376	-0.086277	4.501846
440.950753	6961.219911	15.066381	-0.086283	4.499285
440.981890	6953.246803	15.071386	-0.086283	4.496750
441.015682	6945.233998	15.076391	-0.086284	4.494202
440.719667	6937.242393	15.081395	-0.086224	4.491657
440.900992	6929.234006	15.086400	-0.086253	4.489108
440.922162	6921.264393	15.091405	-0.086251	4.486569
440.992495	6913.155740	15.096410	-0.086259	4.483984
440.647550	6905.311393	15.101415	-0.086190	4.481481
440.576470	6897.201088	15.106419	-0.086171	4.478892
440.616068	6889.280741	15.111424	-0.086173	4.476363
440.343891	6881.199998	15.116429	-0.086117	4.473780
440.923855	6873.205352	15.121434	-0.086220	4.471226
441.416168	6865.147948	15.126439	-0.086307	4.468651
441.519841	6857.124741	15.131443	-0.086321	4.466083
441.393038	6849.186331	15.136448	-0.086292	4.463540
441.364490	6841.229681	15.141453	-0.086281	4.460991
441.113124	6833.191246	15.146458	-0.086229	4.458412
440.862187	6825.254850	15.151463	-0.086177	4.455865
440.783323	6817.242774	15.156467	-0.086157	4.453293
440.691920	6809.280255	15.161472	-0.086135	4.450735
440.957402	6801.119798	15.166477	-0.086179	4.448114
441.077420	6793.097320	15.171482	-0.086196	4.445535
440.913120	6785.198344	15.176487	-0.086161	4.442992
440.727198	6777.159846	15.181491	-0.086121	4.440404
440.622585	6769.244002	15.186496	-0.086096	4.437853
440.347909	6761.248346	15.191501	-0.086040	4.435275
440.411476	6753.171610	15.196506	-0.086046	4.432670
440.237879	6745.159620	15.201511	-0.086009	4.430084
440.424936	6737.115427	15.206515	-0.086038	4.427488
440.210313	6729.162861	15.211520	-0.085993	4.424917
440.222129	6721.156103	15.216525	-0.085990	4.422329
440.397403	6713.095242	15.221530	-0.086018	4.419723
440.636673	6705.163327	15.226535	-0.086057	4.417157
440.220687	6697.106796	15.231539	-0.085974	4.414546
440.173417	6689.169987	15.236544	-0.085960	4.411974
440.157993	6681.131362	15.241549	-0.085952	4.409368
440.036557	6673.141772	15.246554	-0.085924	4.406776
440.166322	6665.088843	15.251559	-0.085943	4.404162
439.773881	6657.236818	15.256563	-0.085865	4.401610
439.686426	6649.208969	15.261568	-0.085843	4.399000
439.811716	6641.192435	15.266573	-0.085861	4.396395
439.633721	6633.164381	15.271578	-0.085823	4.393781
439.729411	6625.221190	15.276583	-0.085836	4.391196
439.229363	6617.169778	15.281587	-0.085737	4.388570
439.303074	6609.233633	15.286592	-0.085746	4.385984
439.230710	6601.175879	15.291597	-0.085727	4.383356
439.350523	6593.182235	15.296602	-0.085744	4.380748
439.341224	6585.145285	15.301607	-0.085737	4.378123
439.719129	6577.125254	15.306611	-0.085802	4.375506
439.676765	6569.149165	15.311616	-0.085789	4.372898
439.522218	6561.158266	15.316621	-0.085755	4.370283
439.156441	6553.232951	15.321626	-0.085682	4.367686
439.509986	6545.181826	15.326631	-0.085743	4.365052
439.131337	6537.266452	15.331635	-0.085667	4.362455
439.501009	6529.203562	15.336640	-0.085730	4.359814
439.186270	6521.306930	15.341645	-0.085667	4.357221
439.008101	6513.223874	15.346650	-0.085628	4.354566
438.929662	6505.225309	15.351655	-0.085608	4.351938
438.994407	6497.096407	15.356659	-0.085615	4.349266
439.171277	6489.192933	15.361664	-0.085643	4.346668
438.694113	6481.175390	15.366669	-0.085549	4.344026
438.572146	6473.247598	15.371674	-0.085521	4.341415
438.742786	6465.223093	15.376679	-0.085547	4.338772
438.450452	6457.242695	15.381683	-0.085488	4.336138
438.472406	6449.243742	15.386688	-0.085487	4.333500
438.274662	6441.229380	15.391693	-0.085445	4.330852
438.361226	6433.214104	15.396698	-0.085455	4.328206
438.222114	6425.184630	15.401703	-0.085424	4.325551
437.912230	6417.248321	15.406707	-0.085361	4.322924
438.325579	6409.206703	15.411712	-0.085433	4.320266
438.619298	6401.182274	15.416717	-0.085483	4.317611
438.358585	6393.224600	15.421722	-0.085429	4.314972
438.596919	6385.200942	15.426727	-0.085468	4.312314
438.256138	6377.184642	15.431731	-0.085399	4.309652
438.153593	6369.187081	15.436736	-0.085375	4.306997
437.985862	6361.175512	15.441741	-0.085338	4.304334
437.606494	6353.211108	15.446746	-0.085263	4.301684
437.831373	6345.184314	15.451751	-0.085299	4.299016
437.562677	6337.201717	15.456755	-0.085244	4.296358
437.885581	6329.147512	15.461760	-0.085299	4.293679
437.834062	6321.137284	15.466765	-0.085284	4.291009
437.793919	6313.140187	15.471770	-0.085271	4.288343
437.976469	6305.141099	15.476775	-0.085300	4.285676
437.610965	6297.197459	15.481779	-0.085227	4.283021
437.952539	6289.183339	15.486784	-0.085285	4.280348
437.506354	6281.222117	15.491789	-0.085197	4.277683
437.692145	6273.165316	15.496794	-0.085226	4.274990
437.454788	6265.196319	15.501799	-0.085177	4.272321
437.502241	6257.112485	15.506803	-0.085180	4.269614
437.765975	6249.182215	15.511808	-0.085224	4.266960
437.193623	6241.159793	15.516813	-0.085112	4.264265
436.885570	6233.224345	15.521818	-0.085050	4.261599
437.187321	6225.150722	15.526823	-0.085101	4.258892
437.035242	6217.188336	15.531827	-0.085067	4.256216
436.943847	6209.133599	15.536832	-0.085045	4.253507
436.552448	6201.163474	15.541837	-0.084967	4.250823
437.194326	6193.099027	15.546842	-0.085081	4.248115
437.046019	6185.106809	15.551847	-0.085048	4.245422
436.974674	6177.117399	15.556851	-0.085030	4.242729
437.183505	6169.139366	15.561856	-0.085063	4.240041
437.400133	6161.134628	15.566861	-0.085099	4.237342
436.765971	6153.212015	15.571866	-0.084975	4.234661
437.331916	6145.135462	15.576871	-0.085075	4.231938
437.130784	6137.071245	15.581875	-0.085033	4.229210
437.125575	6129.138092	15.586880	-0.085027	4.226526
437.070583	6121.087090	15.591885	-0.085011	4.223800
437.186057	6113.135402	15.596890	-0.085027	4.221108
436.873516	6105.164704	15.601895	-0.084964	4.218403
437.107640	6097.116299	15.606899	-0.085002	4.215676
437.085959	6089.143843	15.611904	-0.084993	4.212970
437.168462	6081.106037	15.616909	-0.085003	4.210242
436.699676	6073.164980	15.621914	-0.084911	4.207538
436.872991	6065.124508	15.626919	-0.084938	4.204806
436.692248	6057.178004	15.631923	-0.084899	4.202100
436.681797	6049.155846	15.636928	-0.084892	4.199369
436.247126	6041.228285	15.641933	-0.084806	4.196663
436.634707	6033.078674	15.646938	-0.084872	4.193889
436.562980	6025.138371	15.651943	-0.084854	4.191179
436.223553	6017.124616	15.656947	-0.084785	4.188440
436.302436	6009.088172	15.661952	-0.084795	4.185696
436.216803	6001.123834	15.666957	-0.084774	4.182972
436.000572	5993.151928	15.671962	-0.084728	4.180243
436.029930	5985.193155	15.676967	-0.084728	4.177519
435.782930	5977.119879	15.681971	-0.084677	4.174751
435.923155	5969.117612	15.686976	-0.084698	4.172011
436.205872	5961.018114	15.691981	-0.084745	4.169236
435.774427	5953.156767	15.696986	-0.084660	4.166533
436.352175	5945.076325	15.701991	-0.084762	4.163766
435.831038	5937.166953	15.706995	-0.084660	4.161041
435.709376	5929.182221	15.712000	-0.084632	4.158294
435.823204	5921.131641	15.717005	-0.084648	4.155526
435.756321	5913.154657	15.722010	-0.084630	4.152778
435.946769	5905.144507	15.727015	-0.084661	4.150021
435.557474	5897.142097	15.732019	-0.084583	4.147257
435.463926	5889.148640	15.737024	-0.084560	4.144498
435.220495	5881.223122	15.742029	-0.084510	4.141759
435.155416	5873.149882	15.747034	-0.084492	4.138969
435.317842	5865.181846	15.752039	-0.084517	4.136217
435.481070	5857.104442	15.757043	-0.084543	4.133425
435.720937	5849.091715	15.762048	-0.084582	4.130654
435.802495	5841.099368	15.767053	-0.084592	4.127887
435.411519	5833.127907	15.772058	-0.084514	4.125119
435.105967	5825.241430	15.777063	-0.084452	4.122379
434.934772	5817.171654	15.782067	-0.084415	4.119576
434.784023	5809.248620	15.787072	-0.084381	4.116822
434.607315	5801.197287	15.792077	-0.084343	4.114021
434.922391	5793.133836	15.797082	-0.084397	4.111221
434.972749	5785.118573	15.802087	-0.084401	4.108432
434.484386	5777.186739	15.807091	-0.084305	4.105663
434.386720	5769.172229	15.812096	-0.084281	4.102869
434.734709	5761.106752	15.817101	-0.084341	4.100061
434.646227	5753.133232	15.822106	-0.084319	4.097277
434.873967	5745.067384	15.827111	-0.084356	4.094463
434.797119	5737.123065	15.832115	-0.084337	4.091686
434.667840	5729.143499	15.837120	-0.084307	4.088894
434.332426	5721.195805	15.842125	-0.084240	4.086107
434.451925	5713.126942	15.847130	-0.084257	4.083284
434.783609	5705.124230	15.852135	-0.084313	4.080484
434.633041	5697.119510	15.857139	-0.084280	4.077675
434.508746	5689.168185	15.862144	-0.084252	4.074883
434.532922	5681.177870	15.867149	-0.084251	4.072077
434.063954	5673.183824	15.872154	-0.084158	4.069261
433.900993	5665.186885	15.877159	-0.084123	4.066447
433.558604	5657.196161	15.882163	-0.084054	4.063630
433.560073	5649.226443	15.887168	-0.084049	4.060824
433.927469	5641.155175	15.892173	-0.084112	4.057985
433.494299	5633.187945	15.897178	-0.084026	4.055169
433.922677	5625.164042	15.902183	-0.084101	4.052344
433.524801	5617.127898	15.907187	-0.084021	4.049500
433.757128	5609.113963	15.912192	-0.084059	4.046672
433.351707	5601.175248	15.917197	-0.083979	4.043859
433.565890	5593.150308	15.922202	-0.084013	4.041022
433.427264	5585.191621	15.927207	-0.083982	4.038202
433.576577	5577.137574	15.932211	-0.084005	4.035350
433.582710	5569.137859	15.937216	-0.084001	4.032514
433.291546	5561.115009	15.942221	-0.083941	4.029662
433.455131	5553.100162	15.947226	-0.083967	4.026818
433.709143	5545.080642	15.952231	-0.084009	4.023973
433.054795	5537.206600	15.957235	-0.083882	4.021162
433.035445	5529.234588	15.962240	-0.083873	4.018325
432.794756	5521.229371	15.967245	-0.083823	4.015470
433.003307	5513.211741	15.972250	-0.083856	4.012616
432.947253	5505.164805	15.977255	-0.083841	4.009745
432.805653	5497.165267	15.982259	-0.083809	4.006888
432.997035	5489.142753	15.987264	-0.083839	4.004026
433.179506	5481.196181	15.992269	-0.083868	4.001189
432.852038	5473.208644	15.997274	-0.083802	3.998327
432.506100	5465.288889	16.002279	-0.083732	3.995487
432.309524	5457.270195	16.007283	-0.083691	3.992611
432.410915	5449.180389	16.012288	-0.083704	3.989713
432.390025	5441.198893	16.017293	-0.083695	3.986850
432.667122	5433.140924	16.022298	-0.083741	3.983963
433.011838	5425.149701	16.027303	-0.083800	3.981098
432.674283	5417.199935	16.032307	-0.083732	3.978235
432.481805	5409.245476	16.037312	-0.083691	3.975370
433.024411	5401.145437	16.042317	-0.083787	3.972464
432.580110	5393.169929	16.047322	-0.083699	3.969583
432.871307	5385.215080	16.052327	-0.083748	3.966720
432.505174	5377.204226	16.057331	-0.083675	3.963824
432.415466	5369.273773	16.062336	-0.083653	3.960959
432.725376	5361.219388	16.067341	-0.083705	3.958054
432.731970	5353.185175	16.072346	-0.083701	3.955150
432.877130	5345.180065	16.077351	-0.083723	3.952256
432.264077	5337.199348	16.082355	-0.083604	3.949355
432.210026	5329.246290	16.087360	-0.083588	3.946472
432.428699	5321.158639	16.092365	-0.083624	3.943543
432.350550	5313.189298	16.097370	-0.083604	3.940650
432.493351	5305.192144	16.102375	-0.083625	3.937748
432.030507	5297.267304	16.107379	-0.083534	3.934860
431.967403	5289.235959	16.112384	-0.083517	3.931937
431.879535	5281.199044	16.117389	-0.083495	3.929010
431.729890	5273.237362	16.122394	-0.083462	3.926108
431.445193	5265.275873	16.127399	-0.083404	3.923200
431.846048	5257.158595	16.132403	-0.083473	3.920247
431.584228	5249.284860	16.137408	-0.083420	3.917367
431.692238	5241.235129	16.142413	-0.083434	3.914428
431.623314	5233.227274	16.147418	-0.083416	3.911499
431.856473	5225.237480	16.152423	-0.083455	3.908581
431.643980	5217.230554	16.157427	-0.083410	3.905645
431.582300	5209.256559	16.162432	-0.083393	3.902722
431.646928	5201.235799	16.167437	-0.083400	3.899782
432.102105	5193.189716	16.172442	-0.083479	3.896838
431.545724	5185.320060	16.177447	-0.083371	3.893937
431.411611	5177.269606	16.182451	-0.083340	3.890975
431.903202	5169.216556	16.187456	-0.083427	3.888023
431.418418	5161.295107	16.192461	-0.083331	3.885097
431.456076	5153.270563	16.197466	-0.083333	3.882142
431.836072	5145.267047	16.202471	-0.083398	3.879199
431.517090	5137.369993	16.207475	-0.083334	3.876279
431.345041	5129.289966	16.212480	-0.083297	3.873292
431.328729	5121.145893	16.217485	-0.083288	3.870283
431.501195	5113.146114	16.222490	-0.083315	3.867328
431.409906	5105.203487	16.227495	-0.083293	3.864387
431.150621	5097.249475	16.232499	-0.083239	3.861436
431.841961	5089.162751	16.237504	-0.083363	3.858453
431.242287	5081.296744	16.242509	-0.083246	3.855523
431.305493	5073.278099	16.247514	-0.083253	3.852547
430.738935	5065.336962	16.252519	-0.083142	3.849585
430.724131	5057.308380	16.257523	-0.083134	3.846600
430.807439	5049.242645	16.262528	-0.083144	3.843601
431.540460	5041.238633	16.267533	-0.083275	3.840636
431.063954	5033.309833	16.272538	-0.083181	3.837671
430.833651	5025.368857	16.277543	-0.083133	3.834704
430.615937	5017.326369	16.282547	-0.083088	3.831698
430.794043	5009.287150	16.287552	-0.083116	3.828699
430.899367	5001.293501	16.292557	-0.083130	3.825713
430.904069	4993.268613	16.297562	-0.083126	3.822711
430.780913	4985.350956	16.302567	-0.083097	3.819744
430.928451	4977.295174	16.307571	-0.083120	3.816729
431.045210	4969.268340	16.312576	-0.083136	3.813721
430.919671	4961.305515	16.317581	-0.083108	3.810730
430.859859	4953.306841	16.322586	-0.083091	3.807724
430.808194	4945.308213	16.327591	-0.083076	3.804717
430.501902	4937.378591	16.332595	-0.083014	3.801727
430.991273	4929.301075	16.337600	-0.083100	3.798697
430.969060	4921.353633	16.342605	-0.083091	3.795702
430.890723	4913.318241	16.347610	-0.083071	3.792670
430.879182	4905.353042	16.352615	-0.083063	3.789664
431.025868	4897.308454	16.357619	-0.083085	3.786629
431.006109	4889.303613	16.362624	-0.083077	3.783603
430.630458	4881.384899	16.367629	-0.083001	3.780599
430.570958	4873.356636	16.372634	-0.082985	3.777558
430.262088	4865.430248	16.377639	-0.082922	3.774547
430.368180	4857.366793	16.382643	-0.082937	3.771492
430.079918	4849.420813	16.387648	-0.082878	3.768470
430.696218	4841.298937	16.392653	-0.082987	3.765399
430.099978	4833.424666	16.397658	-0.082871	3.762392
430.137385	4825.419382	16.402663	-0.082873	3.759347
429.733210	4817.468996	16.407667	-0.082793	3.756311
429.958546	4809.423858	16.412672	-0.082829	3.753250
430.051721	4801.405875	16.417677	-0.082841	3.750195
430.139789	4793.380000	16.422682	-0.082853	3.747134
430.112362	4785.395007	16.427687	-0.082842	3.744083
429.914328	4777.463414	16.432691	-0.082800	3.741046
430.062096	4769.409232	16.437696	-0.082822	3.737968
429.511106	4761.503752	16.442701	-0.082715	3.734927
429.726769	4753.445347	16.447706	-0.082750	3.731844
429.771427	4745.426595	16.452711	-0.082753	3.728770
429.350788	4737.456972	16.457715	-0.082669	3.725700
429.482056	4729.453960	16.462720	-0.082688	3.722628
429.650363	4721.399884	16.467725	-0.082714	3.719536
429.526637	4713.473012	16.472730	-0.082686	3.716482
429.584189	4705.453249	16.477735	-0.082692	3.713395
429.320179	4697.389360	16.482739	-0.082637	3.710279
428.830247	4689.479208	16.487744	-0.082541	3.707215
428.174286	4681.527060	16.492749	-0.082413	3.704128
428.164271	4673.575064	16.497754	-0.082406	3.701055
428.567303	4665.442275	16.502759	-0.082476	3.697919
428.662638	4657.413455	16.507763	-0.082489	3.694814
428.584943	4649.471465	16.512768	-0.082469	3.691735
429.037165	4641.378832	16.517773	-0.082548	3.688609
428.870261	4633.423244	16.522778	-0.082512	3.685517
428.668914	4625.524960	16.527783	-0.082469	3.682444
428.274686	4617.539726	16.532787	-0.082390	3.679330
428.588122	4609.525940	16.537792	-0.082443	3.676220
428.974156	4601.428877	16.542797	-0.082510	3.673078
428.325038	4593.542597	16.547802	-0.082384	3.669987
428.227893	4585.574034	16.552807	-0.082361	3.666876
428.461811	4577.487094	16.557811	-0.082399	3.663725
427.986731	4569.615061	16.562816	-0.082305	3.660637
427.747860	4561.599416	16.567821	-0.082256	3.657496
428.346242	4553.462288	16.572826	-0.082362	3.654327
428.293793	4545.530368	16.577831	-0.082347	3.651219
427.762938	4537.575858	16.582835	-0.082243	3.648085
428.593945	4529.458023	16.587840	-0.082392	3.644923
428.798029	4521.511797	16.592845	-0.082425	3.641808
428.555043	4513.549075	16.597850	-0.082375	3.638671
428.969410	4505.530922	16.602855	-0.082446	3.635528
428.388038	4497.615585	16.607859	-0.082333	3.632395
428.704994	4489.568951	16.612864	-0.082387	3.629233
428.545940	4481.601152	16.617869	-0.082352	3.626086
428.312151	4473.585623	16.622874	-0.082303	3.622915
428.027773	4465.659831	16.627879	-0.082245	3.619775
428.119116	4457.611427	16.632883	-0.082257	3.616594
427.581275	4449.699043	16.637888	-0.082151	3.613447
427.135487	4441.691829	16.642893	-0.082063	3.610262
427.185039	4433.637061	16.647898	-0.082067	3.607069
427.445840	4425.601559	16.652903	-0.082111	3.603888
427.375712	4417.660813	16.657907	-0.082092	3.600732
427.582780	4409.633013	16.662912	-0.082126	3.597546
427.501506	4401.635733	16.667917	-0.082105	3.594361
427.209926	4393.672016	16.672922	-0.082046	3.591181
427.182192	4385.647506	16.677927	-0.082035	3.587981
427.225273	4377.615553	16.682931	-0.082038	3.584777
427.166621	4369.667069	16.687936	-0.082022	3.581601
427.101442	4361.674626	16.692941	-0.082005	3.578405
427.204746	4353.674468	16.697946	-0.082019	3.575207
427.712072	4345.631768	16.702951	-0.082108	3.572002
427.115529	4337.679500	16.707955	-0.081992	3.568797
427.248661	4329.697764	16.712960	-0.082011	3.565599
427.385967	4321.713493	16.717965	-0.082031	3.562397
427.086518	4313.714945	16.722970	-0.081970	3.559174
427.282340	4305.801136	16.727975	-0.082002	3.555997
426.935037	4297.709954	16.732979	-0.081932	3.552729
427.283142	4289.633902	16.737984	-0.081991	3.549485
427.170692	4281.681429	16.742989	-0.081965	3.546274
426.645487	4273.759259	16.747994	-0.081862	3.543059
426.720386	4265.760699	16.752999	-0.081871	3.539830
426.732152	4257.723337	16.758003	-0.081868	3.536579
427.356593	4249.648492	16.763008	-0.081979	3.533330
426.659869	4241.800630	16.768013	-0.081844	3.530128
425.896039	4233.873840	16.773018	-0.081697	3.526890
426.372573	4225.773883	16.778023	-0.081780	3.523616
426.546707	4217.769274	16.783027	-0.081807	3.520370
426.137444	4209.880389	16.788032	-0.081726	3.517148
425.669200	4201.903877	16.793037	-0.081633	3.513886
426.201943	4193.807529	16.798042	-0.081727	3.510605
425.995546	4185.817900	16.803047	-0.081684	3.507340
426.367948	4177.716075	16.808051	-0.081748	3.504044
426.449613	4169.782895	16.813056	-0.081758	3.500806
426.460255	4161.804654	16.818061	-0.081755	3.497543
426.606919	4153.759032	16.823066	-0.081777	3.494254
426.751006	4145.820897	16.828071	-0.081798	3.491007
426.502838	4137.864292	16.833075	-0.081747	3.487735
425.720819	4129.947293	16.838080	-0.081596	3.484460
425.894339	4121.960797	16.843085	-0.081623	3.481184
425.980375	4113.901515	16.848090	-0.081634	3.477872
426.001578	4105.907396	16.853095	-0.081633	3.474582
425.715475	4097.943370	16.858099	-0.081574	3.471290
425.883702	4089.867064	16.863104	-0.081600	3.467965
425.913904	4081.869334	16.868109	-0.081601	3.464664
425.825443	4073.897167	16.873114	-0.081579	3.461367
425.483298	4065.963872	16.878119	-0.081510	3.458073
425.300129	4057.969543	16.883123	-0.081471	3.454757
425.638138	4049.918485	16.888128	-0.081528	3.451432
425.100001	4041.993557	16.893133	-0.081423	3.448126
425.036158	4033.948802	16.898138	-0.081406	3.444783
424.906680	4026.048684	16.903143	-0.081377	3.441495
424.701287	4018.034197	16.908147	-0.081333	3.438154
424.750459	4010.005770	16.913152	-0.081337	3.434812
424.681428	4002.051094	16.918157	-0.081319	3.431494
424.394724	3994.034017	16.923162	-0.081260	3.428138
424.801861	3985.985735	16.928167	-0.081331	3.424791
424.682637	3978.015262	16.933171	-0.081303	3.421455
424.483636	3970.060801	16.938176	-0.081261	3.418119
423.989642	3962.121102	16.943181	-0.081164	3.414775
424.116049	3954.047143	16.948186	-0.081182	3.411394
424.354840	3946.019975	16.953191	-0.081221	3.408033
423.841754	3938.070888	16.958195	-0.081121	3.404675
423.813965	3930.122142	16.963200	-0.081110	3.401331
424.057335	3922.096672	16.968205	-0.081150	3.397961
424.039312	3914.067248	16.973210	-0.081142	3.394577
423.872335	3906.094805	16.978215	-0.081106	3.391208
424.047690	3898.025706	16.983219	-0.081133	3.387807
423.552443	3890.114407	16.988224	-0.081035	3.384446
423.949890	3882.065173	16.993229	-0.081104	3.381055
423.815553	3874.093943	16.998234	-0.081074	3.377674
423.944150	3866.090401	17.003239	-0.081093	3.374285
423.590529	3858.142439	17.008243	-0.081022	3.370900
423.547179	3850.148555	17.013248	-0.081008	3.367502
423.409867	3842.181202	17.018253	-0.080978	3.364109
424.031525	3834.092814	17.023258	-0.081088	3.360689
424.232608	3826.090820	17.028263	-0.081120	3.357287
423.976189	3818.148570	17.033267	-0.081067	3.353890
424.225792	3810.168671	17.038272	-0.081109	3.350493
423.595286	3802.271887	17.043277	-0.080986	3.347094
423.791209	3794.201982	17.048282	-0.081017	3.343649
423.897194	3786.229119	17.053287	-0.081032	3.340238
423.512620	3778.292452	17.058291	-0.080955	3.336821
423.512622	3770.277663	17.063296	-0.080950	3.333382
423.711310	3762.241154	17.068301	-0.080981	3.329937
423.090228	3754.331561	17.073306	-0.080861	3.326512
423.164068	3746.328551	17.078311	-0.080869	3.323070
423.184600	3738.301639	17.083315	-0.080868	3.319611
423.421054	3730.313650	17.088320	-0.080907	3.316175
423.160125	3722.335139	17.093325	-0.080853	3.312719
422.593648	3714.378142	17.098330	-0.080742	3.309258
423.143003	3706.311091	17.103335	-0.080839	3.305788
423.020958	3698.315808	17.108339	-0.080811	3.302320
422.748923	3690.374234	17.113344	-0.080755	3.298865
422.951468	3682.373599	17.118349	-0.080788	3.295400
422.684965	3674.370813	17.123354	-0.080733	3.291912
422.597348	3666.381855	17.128359	-0.080711	3.288433
422.488034	3658.364687	17.133363	-0.080686	3.284937
422.801637	3650.400425	17.138368	-0.080739	3.281478
422.735265	3642.442089	17.143373	-0.080721	3.278002
423.145664	3634.359837	17.148378	-0.080793	3.274488
423.130774	3626.445822	17.153383	-0.080785	3.271026
422.557806	3618.464847	17.158387	-0.080673	3.267509
422.428849	3610.468050	17.163392	-0.080643	3.263999
421.796295	3602.594878	17.168397	-0.080521	3.260519
421.758744	3594.598426	17.173402	-0.080508	3.257005
421.820483	3586.557385	17.178407	-0.080515	3.253472
421.917890	3578.475650	17.183411	-0.080527	3.249918
422.064932	3570.501451	17.188416	-0.080550	3.246410
421.891384	3562.550271	17.193421	-0.080512	3.242896
421.830045	3554.538623	17.198426	-0.080495	3.239355
422.017012	3546.594990	17.203431	-0.080525	3.235851
421.963966	3538.571808	17.208435	-0.080510	3.232298
422.294636	3530.499406	17.213440	-0.080566	3.228735
422.697588	3522.464089	17.218445	-0.080636	3.225188
422.456143	3514.547714	17.223450	-0.080586	3.221662
422.270014	3506.613109	17.228455	-0.080546	3.218127
421.752558	3498.685209	17.233459	-0.080444	3.214577
422.410074	3490.576483	17.238464	-0.080562	3.210993
422.054427	3482.646108	17.243469	-0.080490	3.207440
421.726543	3474.657746	17.248474	-0.080424	3.203859
422.037133	3466.656284	17.253479	-0.080477	3.200296
421.820723	3458.682896	17.258483	-0.080431	3.196718
421.383462	3450.754454	17.263488	-0.080344	3.193147
421.295220	3442.764525	17.268493	-0.080323	3.189560
421.636929	3434.666982	17.273498	-0.080381	3.185939
421.403644	3426.761942	17.278503	-0.080332	3.182375
421.486417	3418.736719	17.283507	-0.080343	3.178767
422.048622	3410.688443	17.288512	-0.080442	3.175165
421.487692	3402.808375	17.293517	-0.080332	3.171586
421.561207	3394.741434	17.298522	-0.080341	3.167947
421.754850	3386.754095	17.303527	-0.080372	3.164344
421.357846	3378.873006	17.308531	-0.080293	3.160760
421.263817	3370.874869	17.313536	-0.080270	3.157131
421.693868	3362.821973	17.318541	-0.080345	3.153497
421.389058	3354.858233	17.323546	-0.080283	3.149867
421.935208	3346.793602	17.328551	-0.080379	3.146224
420.888223	3338.957580	17.333555	-0.080179	3.142610
420.869580	3330.918101	17.338560	-0.080170	3.138945
421.157643	3322.908118	17.343565	-0.080219	3.135303
421.058268	3314.887856	17.348570	-0.080195	3.131635
421.311563	3306.871164	17.353575	-0.080237	3.127980
421.003649	3298.918503	17.358579	-0.080174	3.124324
420.800974	3291.010359	17.363584	-0.080132	3.120690
420.789706	3283.027045	17.368589	-0.080124	3.117025
421.217677	3274.917260	17.373594	-0.080199	3.113318
421.231042	3266.969269	17.378599	-0.080196	3.109662
420.757009	3259.045308	17.383603	-0.080102	3.105991
421.091270	3251.017351	17.388608	-0.080159	3.102304
420.950835	3243.066504	17.393613	-0.080128	3.098627
421.177731	3235.002124	17.398618	-0.080165	3.094910
420.718930	3227.149933	17.403623	-0.080074	3.091254
420.776726	3219.105087	17.408627	-0.080080	3.087529
420.147000	3211.179854	17.413632	-0.079958	3.083823
420.104355	3203.216463	17.418637	-0.079944	3.080122
420.393392	3195.152832	17.423642	-0.079993	3.076386
420.409558	3187.138282	17.428647	-0.079991	3.072655
420.204332	3179.120780	17.433651	-0.079947	3.068908
420.500129	3171.094255	17.438656	-0.079997	3.065176
420.673299	3163.132761	17.443661	-0.080024	3.061464
420.741505	3155.130351	17.448666	-0.080032	3.057723
420.448266	3147.213824	17.453671	-0.079972	3.054000
420.178566	3139.271393	17.458675	-0.079916	3.050262
420.241052	3131.256416	17.463680	-0.079923	3.046501
420.258343	3123.264648	17.468685	-0.079921	3.042744
420.045893	3115.305424	17.473690	-0.079876	3.038987
420.360549	3107.302295	17.478695	-0.079929	3.035230
419.914211	3099.362286	17.483699	-0.079841	3.031461
420.442380	3091.277820	17.488704	-0.079934	3.027667
420.523453	3083.289192	17.493709	-0.079944	3.023892
419.959791	3075.418675	17.498714	-0.079834	3.020135
419.749459	3067.475520	17.503719	-0.079790	3.016358
419.793872	3059.429396	17.508723	-0.079793	3.012539
419.601684	3051.436917	17.513728	-0.079752	3.008729
419.862296	3043.425562	17.518733	-0.079795	3.004928
419.862165	3035.463742	17.523738	-0.079790	3.001132
419.963247	3027.492053	17.528743	-0.079803	2.997332
419.991374	3019.458568	17.533747	-0.079803	2.993494
419.772997	3011.515867	17.538752	-0.079757	2.989682
419.836972	3003.524490	17.543757	-0.079764	2.985857
420.089533	2995.485350	17.548762	-0.079806	2.982013
419.908670	2987.573223	17.553767	-0.079767	2.978203
419.781168	2979.565022	17.558771	-0.079738	2.974344
420.020529	2971.554877	17.563776	-0.079777	2.970499
419.823854	2963.594382	17.568781	-0.079736	2.966650
419.883948	2955.604222	17.573786	-0.079741	2.962795
419.640711	2947.705756	17.578791	-0.079691	2.958963
419.747760	2939.698356	17.583795	-0.079706	2.955092
419.334239	2931.731073	17.588800	-0.079624	2.951208
419.919453	2923.680927	17.593805	-0.079727	2.947332
419.462679	2915.743429	17.598810	-0.079637	2.943449
419.192247	2907.830213	17.603815	-0.079581	2.939584
419.287028	2899.810015	17.608819	-0.079594	2.935680
419.146872	2891.809634	17.613824	-0.079563	2.931769
419.261819	2883.791279	17.618829	-0.079579	2.927857
418.861542	2875.842320	17.623834	-0.079499	2.923946
419.259206	2867.851070	17.628839	-0.079568	2.920052
419.251239	2859.867468	17.633843	-0.079561	2.916135
418.838828	2851.897526	17.638848	-0.079479	2.912197
418.848422	2843.896788	17.643853	-0.079476	2.908262
418.664903	2835.890360	17.648858	-0.079436	2.904308
418.684334	2827.953272	17.653863	-0.079435	2.900394
418.510745	2819.976433	17.658867	-0.079397	2.896444
418.669132	2811.964608	17.663872	-0.079421	2.892490
418.541840	2803.993770	17.668877	-0.079392	2.888535
418.412603	2795.987587	17.673882	-0.079363	2.884557
418.635247	2788.030223	17.678887	-0.079399	2.880618
418.241967	2780.110959	17.683891	-0.079321	2.876657
418.193779	2772.114396	17.688896	-0.079307	2.872672
417.879418	2764.169669	17.693901	-0.079243	2.868692
417.766715	2756.147719	17.698906	-0.079217	2.864679
417.728893	2748.198446	17.703911	-0.079205	2.860701
417.816009	2740.152617	17.708915	-0.079216	2.856677
417.764044	2732.202330	17.713920	-0.079201	2.852687
417.705415	2724.209911	17.718925	-0.079185	2.848669
417.503207	2716.243330	17.723930	-0.079142	2.844651
417.757684	2708.270578	17.728935	-0.079184	2.840650
417.689892	2700.298824	17.733939	-0.079166	2.836625
417.560030	2692.328865	17.738944	-0.079137	2.832592
417.899700	2684.282438	17.743949	-0.079195	2.828542
417.709425	2676.304665	17.748954	-0.079154	2.824490
417.634323	2668.370674	17.753959	-0.079135	2.820461
417.388490	2660.420494	17.758963	-0.079084	2.816408
416.814486	2652.510666	17.763968	-0.078972	2.812351
417.162651	2644.424857	17.768973	-0.079031	2.808252
417.069100	2636.439851	17.773978	-0.079009	2.804172
417.154110	2628.509252	17.778983	-0.079019	2.800125
416.942521	2620.535603	17.783987	-0.078975	2.796032
417.210834	2612.494618	17.788992	-0.079019	2.791928
417.049319	2604.563565	17.793997	-0.078984	2.787848
417.337359	2596.507817	17.799002	-0.079033	2.783725
416.912568	2588.654101	17.804007	-0.078948	2.779657
416.754035	2580.671906	17.809011	-0.078914	2.775533
417.079835	2572.621116	17.814016	-0.078969	2.771397
416.919293	2564.666623	17.819021	-0.078934	2.767274
416.477157	2556.745860	17.824026	-0.078846	2.763146
416.424255	2548.801392	17.829031	-0.078831	2.759023
416.559463	2540.765458	17.834035	-0.078851	2.754858
416.045809	2532.828757	17.839040	-0.078750	2.750698
415.806783	2524.865136	17.844045	-0.078701	2.746535
416.448900	2516.732331	17.849050	-0.078815	2.742332
416.230033	2508.832464	17.854055	-0.078769	2.738191
416.186557	2500.829541	17.859059	-0.078756	2.734000
416.437307	2492.828728	17.864064	-0.078797	2.729823
416.425753	2484.882131	17.869069	-0.078790	2.725651
416.345311	2476.916805	17.874074	-0.078770	2.721458
416.263269	2469.004278	17.879079	-0.078749	2.717287
415.823294	2461.080173	17.884083	-0.078662	2.713080
415.485617	2453.127926	17.889088	-0.078594	2.708859
414.875472	2445.207010	17.894093	-0.078475	2.704630
415.588975	2437.068111	17.899098	-0.078603	2.700363
415.605493	2429.117786	17.904103	-0.078601	2.696145
415.415577	2421.157392	17.909107	-0.078560	2.691902
415.570492	2413.141971	17.914112	-0.078584	2.687645
415.734823	2405.153808	17.919117	-0.078609	2.683397
415.399903	2397.229706	17.924122	-0.078542	2.679143
414.884748	2389.377710	17.929127	-0.078440	2.674910
415.264572	2381.281100	17.934131	-0.078506	2.670597
414.939717	2373.340619	17.939136	-0.078440	2.666315
415.393702	2365.283300	17.944141	-0.078519	2.662015
415.201452	2357.353476	17.949146	-0.078479	2.657733
414.628680	2349.481049	17.954151	-0.078367	2.653450
414.216287	2341.520745	17.959155	-0.078285	2.649124
414.687726	2333.446998	17.964160	-0.078367	2.644788
414.800473	2325.495611	17.969165	-0.078383	2.640487
414.372053	2317.578712	17.974170	-0.078298	2.636161
414.358020	2309.599277	17.979175	-0.078290	2.631822
414.210458	2301.641285	17.984179	-0.078258	2.627479
413.992527	2293.660965	17.989184	-0.078212	2.623111
413.896572	2285.704272	17.994189	-0.078189	2.618758
414.038886	2277.658739	17.999194	-0.078210	2.614365
414.332926	2269.647511	18.004199	-0.078259	2.609993
414.292019	2261.681795	18.009203	-0.078247	2.605616
414.195338	2253.760012	18.014208	-0.078223	2.601253
414.760691	2245.710698	18.019213	-0.078323	2.596857
414.271507	2237.781283	18.024218	-0.078227	2.592447
414.133854	2229.769463	18.029223	-0.078196	2.588008
414.139668	2221.785757	18.034227	-0.078192	2.583588
413.845497	2213.881161	18.039232	-0.078132	2.579182
413.460300	2206.010180	18.044237	-0.078055	2.574781
413.423739	2198.015118	18.049242	-0.078043	2.570328
413.840889	2189.950332	18.054247	-0.078116	2.565861
413.288121	2182.081254	18.059251	-0.078008	2.561426
413.836397	2174.022976	18.064256	-0.078104	2.556956
413.559617	2166.134558	18.069261	-0.078048	2.552515
413.474385	2158.115582	18.074266	-0.078027	2.548006
413.760461	2150.096913	18.079271	-0.078075	2.543516
413.651747	2142.177658	18.084275	-0.078049	2.539046
413.332875	2134.279196	18.089280	-0.077985	2.534564
413.086555	2126.340895	18.094285	-0.077934	2.530057
413.141138	2118.315954	18.099290	-0.077939	2.525515
413.644598	2110.284950	18.104295	-0.078027	2.520994
413.561880	2102.363699	18.109299	-0.078007	2.516485
413.256023	2094.437060	18.114304	-0.077944	2.511948
413.191899	2086.487628	18.119309	-0.077927	2.507407
412.973340	2078.506893	18.124314	-0.077881	2.502829
412.783570	2070.572284	18.129319	-0.077841	2.498271
413.817041	2062.423659	18.134323	-0.078028	2.493672
413.453783	2054.534473	18.139328	-0.077955	2.489111
413.090512	2046.649137	18.144333	-0.077882	2.484543
413.047385	2038.696169	18.149338	-0.077869	2.479951
412.656671	2030.829577	18.154343	-0.077791	2.475375
412.134870	2022.907944	18.159347	-0.077689	2.470748
412.474001	2014.813287	18.164352	-0.077747	2.466078
412.735873	2006.823577	18.169357	-0.077790	2.461454
412.475115	1998.886122	18.174362	-0.077737	2.456812
412.717582	1990.886575	18.179367	-0.077776	2.452163
412.754708	1982.909117	18.184371	-0.077778	2.447503
412.843336	1974.932827	18.189376	-0.077789	2.442838
412.428519	1967.073934	18.194381	-0.077707	2.438195
412.488605	1959.070785	18.199386	-0.077713	2.433494
412.443140	1951.112415	18.204391	-0.077699	2.428803
412.044067	1943.171249	18.209395	-0.077620	2.424085
411.879600	1935.223010	18.214400	-0.077584	2.419371
412.279285	1927.200428	18.219405	-0.077653	2.414650
411.467614	1919.364407	18.224410	-0.077497	2.409933
411.416010	1911.385759	18.229415	-0.077482	2.405183
411.236974	1903.445712	18.234419	-0.077444	2.400436
411.631432	1895.382191	18.239424	-0.077512	2.395652
411.550843	1887.451183	18.244429	-0.077492	2.390900
411.476438	1879.460252	18.249434	-0.077472	2.386103
411.171307	1871.602926	18.254439	-0.077411	2.381358
411.305066	1863.584156	18.259443	-0.077430	2.376541
411.743731	1855.517629	18.264448	-0.077507	2.371711
411.711308	1847.612969	18.269453	-0.077495	2.366930
411.466177	1839.694130	18.274458	-0.077445	2.362114
411.257202	1831.804933	18.279463	-0.077401	2.357309
411.442755	1823.801200	18.284467	-0.077430	2.352457
411.263337	1815.850167	18.289472	-0.077391	2.347596
411.146035	1807.922060	18.294477	-0.077364	2.342745
411.427532	1799.886497	18.299482	-0.077411	2.337851
411.470893	1791.953986	18.304487	-0.077414	2.332990
411.275472	1784.017076	18.309491	-0.077373	2.328097
410.946405	1776.112490	18.314496	-0.077306	2.323201
411.384327	1768.100900	18.319501	-0.077383	2.318294
411.122719	1760.196730	18.324506	-0.077329	2.313384
410.737174	1752.297866	18.329511	-0.077252	2.308456
410.478307	1744.351473	18.334515	-0.077198	2.303498
410.512028	1736.396282	18.339520	-0.077199	2.298550
410.403081	1728.453891	18.344525	-0.077174	2.293586
410.223880	1720.470869	18.349530	-0.077135	2.288580
410.538980	1712.475554	18.354535	-0.077189	2.283599
410.252144	1704.593592	18.359539	-0.077130	2.278625
410.229685	1696.618959	18.364544	-0.077121	2.273605
410.509292	1688.577161	18.369549	-0.077168	2.268558
410.370691	1680.618934	18.374554	-0.077137	2.263516
410.155176	1672.734292	18.379559	-0.077091	2.258503
409.915550	1664.807047	18.384563	-0.077042	2.253449
410.040529	1656.811716	18.389568	-0.077060	2.248373
409.947034	1648.885711	18.394573	-0.077037	2.243310
410.163200	1640.900568	18.399578	-0.077072	2.238225
410.408306	1632.932991	18.404583	-0.077112	2.233143
409.725126	1625.107804	18.409587	-0.076980	2.228057
409.384428	1617.187804	18.414592	-0.076911	2.222929
409.626950	1609.187647	18.419597	-0.076951	2.217791
409.451136	1601.255013	18.424602	-0.076913	2.212646
409.017175	1593.378875	18.429607	-0.076828	2.207502
408.814996	1585.434092	18.434611	-0.076785	2.202322
408.749114	1577.485455	18.439616	-0.076767	2.197141
408.645406	1569.550457	18.444621	-0.076743	2.191952
408.683060	1561.542001	18.449626	-0.076745	2.186717
408.894101	1553.554155	18.454631	-0.076779	2.181498
409.071418	1545.597886	18.459635	-0.076806	2.176285
408.944643	1537.658976	18.464640	-0.076778	2.171042
408.729426	1529.741573	18.469645	-0.076732	2.165792
408.538084	1521.821958	18.474650	-0.076692	2.160530
408.953623	1513.828223	18.479655	-0.076764	2.155263
409.123167	1505.854788	18.484659	-0.076790	2.149974
408.918633	1497.946627	18.489664	-0.076747	2.144680
408.977955	1490.034857	18.494669	-0.076753	2.139395
408.489700	1482.177029	18.499674	-0.076657	2.134081
408.739802	1474.181805	18.504679	-0.076698	2.128732
408.709900	1466.237886	18.509683	-0.076687	2.123377
408.324229	1458.397549	18.514688	-0.076610	2.118044
408.612517	1450.375550	18.519693	-0.076659	2.112641
408.503179	1442.417261	18.524698	-0.076633	2.107227
408.795207	1434.419597	18.529703	-0.076682	2.101813
408.854721	1426.482960	18.534707	-0.076688	2.096403
409.318257	1418.481258	18.539712	-0.076769	2.090976
409.100741	1410.621974	18.544717	-0.076724	2.085563
408.815567	1402.751399	18.549722	-0.076665	2.080122
408.347298	1394.909608	18.554727	-0.076573	2.074668
408.311707	1386.981925	18.559731	-0.076561	2.069184
407.861208	1379.085467	18.564736	-0.076472	2.063665
407.915404	1371.148510	18.569741	-0.076477	2.058154
408.162654	1363.129665	18.574746	-0.076518	2.052591
408.294765	1355.192560	18.579751	-0.076537	2.047059
407.604687	1347.369654	18.584755	-0.076404	2.041506
407.527904	1339.436588	18.589760	-0.076384	2.035924
408.079866	1331.410761	18.594765	-0.076482	2.030327
407.781506	1323.512724	18.599770	-0.076421	2.024717
407.473622	1315.648763	18.604775	-0.076359	2.019113
407.340456	1307.732010	18.609779	-0.076329	2.013475
407.465024	1299.756798	18.614784	-0.076347	2.007807
407.770626	1291.765503	18.619789	-0.076398	2.002130
408.132883	1283.792953	18.624794	-0.076460	1.996456
407.545282	1276.002975	18.629799	-0.076346	1.990797
407.272164	1268.108838	18.634803	-0.076290	1.985079
406.985017	1260.218163	18.639808	-0.076231	1.979346
407.193552	1252.265206	18.644813	-0.076265	1.973605
406.979233	1244.353292	18.649818	-0.076220	1.967831
406.683187	1236.490262	18.654823	-0.076160	1.962066
407.326116	1228.432350	18.659827	-0.076274	1.956245
407.149157	1220.550065	18.664832	-0.076236	1.950445
407.137180	1212.627081	18.669837	-0.076229	1.944617
406.599913	1204.812734	18.674842	-0.076123	1.938792
406.637512	1196.872311	18.679847	-0.076125	1.932921
406.907360	1188.864146	18.684851	-0.076170	1.927007
406.851766	1180.962842	18.689856	-0.076155	1.921118
407.062958	1173.028862	18.694861	-0.076189	1.915217
406.665474	1165.187963	18.699866	-0.076110	1.909299
406.191144	1157.348511	18.704871	-0.076016	1.903354
406.902485	1149.296089	18.709875	-0.076143	1.897365
406.895682	1141.391623	18.714880	-0.076137	1.891388
406.979422	1133.472217	18.719885	-0.076147	1.885390
406.531931	1125.659217	18.724890	-0.076059	1.879392
406.286704	1117.813028	18.729895	-0.076008	1.873374
405.666029	1109.974003	18.734899	-0.075888	1.867297
406.018248	1101.957544	18.739904	-0.075948	1.861179
405.823088	1094.103245	18.744909	-0.075906	1.855100
405.681263	1086.182607	18.749914	-0.075875	1.848957
405.503805	1078.315549	18.754919	-0.075837	1.842831
405.836588	1070.343144	18.759923	-0.075893	1.836663
405.671687	1062.451189	18.764928	-0.075858	1.830477
405.749211	1054.541231	18.769933	-0.075867	1.824286
405.812632	1046.618391	18.774938	-0.075873	1.818061
405.679377	1038.764477	18.779943	-0.075843	1.811846
405.913108	1030.805751	18.784947	-0.075882	1.805571
405.866053	1022.934668	18.789952	-0.075868	1.799310
406.073864	1015.023836	18.794957	-0.075901	1.793026
405.980337	1007.099368	18.799962	-0.075879	1.786672
405.880120	999.244719	18.804967	-0.075855	1.780351
405.354606	991.470607	18.809971	-0.075752	1.774018
405.169557	983.594304	18.814976	-0.075712	1.767623
405.550198	975.615983	18.819981	-0.075778	1.761194
405.124884	967.814511	18.824986	-0.075694	1.754782
405.124283	959.934776	18.829991	-0.075689	1.748338
405.157889	952.020029	18.834995	-0.075690	1.741845
404.629647	944.224477	18.840000	-0.075586	1.735353
404.922637	936.273637	18.845005	-0.075636	1.728815
404.910714	928.387597	18.850010	-0.075628	1.722266
404.947352	920.512074	18.855015	-0.075630	1.715708
404.753922	912.665083	18.860019	-0.075589	1.709117
404.941004	904.733447	18.865024	-0.075618	1.702481
404.669141	896.922295	18.870029	-0.075563	1.695859
404.863408	888.981147	18.875034	-0.075594	1.689163
404.971342	881.117739	18.880039	-0.075609	1.682496
404.566123	873.338333	18.885043	-0.075528	1.675804
404.355093	865.474728	18.890048	-0.075484	1.669039
403.983193	857.681986	18.895053	-0.075409	1.662286
403.543755	849.866154	18.900058	-0.075322	1.655475
403.457915	841.998432	18.905063	-0.075301	1.648641
403.574859	834.090715	18.910067	-0.075318	1.641771
403.827335	826.180691	18.915072	-0.075360	1.634889
403.564882	818.338376	18.920077	-0.075306	1.627966
403.483130	810.447675	18.925082	-0.075285	1.620995
404.122588	802.483610	18.930087	-0.075399	1.614032
403.820405	794.697121	18.935091	-0.075338	1.607062
403.473450	786.895903	18.940096	-0.075268	1.600043
403.298639	779.103228	18.945101	-0.075230	1.593025
403.577272	771.167684	18.950106	-0.075277	1.585912
403.041808	763.444552	18.955111	-0.075172	1.578842
403.330639	755.514369	18.960115	-0.075221	1.571672
403.198995	747.694156	18.965120	-0.075191	1.564507
403.193741	739.886127	18.970125	-0.075185	1.557340
402.840139	732.097511	18.975130	-0.075114	1.550105
402.798821	724.264094	18.980135	-0.075101	1.542842
402.448665	716.486455	18.985139	-0.075031	1.535549
402.547527	708.610045	18.990144	-0.075044	1.528198
402.879916	700.720346	18.995149	-0.075101	1.520834
402.366276	692.989271	19.000154	-0.075000	1.513454
402.020909	685.213301	19.005159	-0.074931	1.506021
401.930109	677.392766	19.010163	-0.074909	1.498549
402.176999	669.506736	19.015168	-0.074950	1.491029
402.093709	661.719066	19.020173	-0.074929	1.483513
401.601338	653.989106	19.025178	-0.074833	1.475951
401.468617	646.169781	19.030183	-0.074803	1.468319
401.622158	638.300156	19.035187	-0.074826	1.460645
401.822724	630.438202	19.040192	-0.074858	1.452945
401.994368	622.605954	19.045197	-0.074885	1.445229
402.037902	614.818654	19.050202	-0.074888	1.437495
401.685082	607.106031	19.055207	-0.074818	1.429729
401.627802	599.311930	19.060211	-0.074802	1.421887
401.637834	591.522825	19.065216	-0.074799	1.414018
401.478912	583.771713	19.070221	-0.074764	1.406116
401.675806	575.955992	19.075226	-0.074795	1.398163
401.711975	568.184408	19.080231	-0.074797	1.390182
401.693745	560.401269	19.085235	-0.074789	1.382134
401.503122	552.672906	19.090240	-0.074748	1.374066
401.519754	544.891802	19.095245	-0.074746	1.365931
401.282679	537.201608	19.100250	-0.074697	1.357799
401.251543	529.445470	19.105255	-0.074686	1.349584
401.100075	521.712819	19.110259	-0.074653	1.341322
400.932552	513.986194	19.115264	-0.074617	1.333013
400.783040	506.278616	19.120269	-0.074584	1.324675
401.112393	498.462656	19.125274	-0.074640	1.316254
401.674096	490.542831	19.130279	-0.074739	1.307708
401.672597	482.814893	19.135283	-0.074734	1.299213
401.587455	475.121891	19.140288	-0.074713	1.290685
401.086639	467.529594	19.145293	-0.074615	1.282134
400.703099	459.881310	19.150298	-0.074538	1.273486
400.805261	452.132340	19.155303	-0.074552	1.264757
400.819244	444.434609	19.160307	-0.074550	1.256008
400.260517	436.830836	19.165312	-0.074441	1.247195
400.833651	429.028466	19.170317	-0.074543	1.238311
400.639445	421.380616	19.175322	-0.074501	1.229392
399.986566	413.812863	19.180327	-0.074375	1.220409
399.702023	406.166494	19.185331	-0.074317	1.211341
399.786000	398.455935	19.190336	-0.074327	1.202203
399.543148	390.851814	19.195341	-0.074277	1.193056
399.336028	383.203300	19.200346	-0.074234	1.183791
399.845776	375.449240	19.205351	-0.074324	1.174474
399.274880	367.901508	19.210355	-0.074212	1.165109
399.375034	360.239998	19.215360	-0.074226	1.155669
399.505688	352.561937	19.220365	-0.074245	1.146138
399.206475	344.989923	19.225370	-0.074185	1.136567
399.228509	337.364773	19.230375	-0.074184	1.126917
399.319600	329.747517	19.235379	-0.074196	1.117210
399.103828	322.183497	19.240384	-0.074151	1.107418
398.819042	314.658617	19.245389	-0.074093	1.097574
398.998462	307.030044	19.250394	-0.074121	1.087610
398.585648	299.556896	19.255399	-0.074039	1.077624
398.475137	292.001103	19.260403	-0.074014	1.067504
398.362814	284.461859	19.265408	-0.073988	1.057309
398.430595	276.910103	19.270413	-0.073996	1.047040
397.820220	269.496560	19.275418	-0.073877	1.036698
397.610411	262.002711	19.280423	-0.073833	1.026236
397.708324	254.472373	19.285427	-0.073846	1.015691
397.854161	246.940110	19.290432	-0.073869	1.005044
397.691788	239.508574	19.295437	-0.073834	0.994351
397.509121	232.036955	19.300442	-0.073795	0.983478
396.377066	224.778413	19.305447	-0.073579	0.972553
390.669989	218.263122	19.310451	-0.072512	0.961420
388.438450	211.100087	19.315456	-0.072092	0.950093
387.819455	203.649464	19.320461	-0.071972	0.938620
387.005395	196.256333	19.325466	-0.071816	0.927041
386.461074	188.855547	19.330471	-0.071709	0.915377
385.514752	181.541107	19.335475	-0.071528	0.903587
384.350063	174.287503	19.340480	-0.071307	0.891677
383.916673	166.922126	19.345485	-0.071221	0.879632
382.977617	159.679828	19.350490	-0.071042	0.867476
382.443795	152.393138	19.355495	-0.070937	0.855192
381.347425	145.231488	19.360499	-0.070729	0.842772
380.895326	137.964105	19.365504	-0.070640	0.830180
380.220402	130.774173	19.370509	-0.070509	0.817461
379.404050	123.639493	19.375514	-0.070353	0.804593
378.628637	116.536968	19.380519	-0.070204	0.791588
378.135901	109.405635	19.385523	-0.070107	0.778404
377.543934	102.331572	19.390528	-0.069992	0.765067
376.323752	95.424042	19.395533	-0.069761	0.751597
375.662567	88.418011	19.400538	-0.069633	0.737882
375.129895	81.438881	19.405543	-0.069529	0.724006
374.015801	74.797448	19.410547	-0.069317	0.710331