Thu Mar 11 17:58:02 2021

Number of Points = 3606
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.447136	-0.101684	0.000000	-0.000029	0.733887

3.436418	-0.192547	0.005005	-0.000028	0.733709
3.385537	-0.186631	0.010010	-0.000019	0.733704
3.483703	-0.198748	0.015014	-0.000038	0.733716
3.405424	-0.189937	0.020019	-0.000025	0.733708
3.375410	-0.184865	0.025024	-0.000020	0.733709
3.584965	-0.222335	0.030029	-0.000060	0.733710
3.505187	-0.211763	0.035034	-0.000045	0.733704
3.235992	-0.160016	0.040038	0.000004	0.733713
3.162542	-0.149681	0.045043	0.000017	0.733709
3.451128	-0.203474	0.050048	-0.000038	0.733706
3.152512	-0.147705	0.055053	0.000017	0.733712
3.252310	-0.169809	0.060058	-0.000002	0.733706
3.277154	-0.171951	0.065062	-0.000008	0.733711
2.925115	-0.112981	0.070067	0.000057	0.733706
2.858821	-0.163836	0.075072	0.000069	0.733586
3.276263	-0.328576	0.080077	-0.000010	0.733413
3.215849	-0.322538	0.085082	0.000001	0.733405
3.322296	-0.336413	0.090086	-0.000020	0.733416
3.359353	-0.348404	0.095091	-0.000028	0.733407
3.627549	-0.395984	0.100096	-0.000078	0.733409
3.379448	-0.351101	0.105101	-0.000033	0.733412
3.274175	-0.497437	0.110106	-0.000014	0.733094
3.239237	-0.498635	0.115110	-0.000008	0.733082
3.079826	-0.474821	0.120115	0.000020	0.733074
3.019711	-0.462536	0.125120	0.000031	0.733079
3.095592	-0.476709	0.130125	0.000016	0.733079
2.981608	-0.571699	0.135130	0.000036	0.732857
3.037152	-0.627534	0.140134	0.000025	0.732770
3.088726	-0.641337	0.145139	0.000015	0.732763
3.177262	-0.655866	0.150144	-0.000002	0.732766
2.966397	-0.661995	0.155149	0.000036	0.732683
2.563607	-0.714208	0.160154	0.000110	0.732445
2.543225	-0.706575	0.165158	0.000113	0.732454
2.389981	-0.684942	0.170163	0.000141	0.732445
2.202832	-0.650580	0.175168	0.000175	0.732449
2.305975	-0.786239	0.180173	0.000155	0.732223
2.147648	-0.800957	0.185178	0.000184	0.732141
1.969891	-0.764880	0.190182	0.000216	0.732151
2.091710	-0.789122	0.195187	0.000193	0.732148
2.340239	-0.926055	0.200192	0.000146	0.731970
2.271173	-0.990173	0.205197	0.000158	0.731823
1.941857	-0.935996	0.210202	0.000219	0.731816
2.114955	-0.962754	0.215206	0.000186	0.731826
2.271547	-1.126600	0.220211	0.000156	0.731564
2.101039	-1.122030	0.225216	0.000187	0.731515
2.072240	-1.115201	0.230221	0.000191	0.731520
1.734396	-1.133821	0.235226	0.000253	0.731369
1.512293	-1.177610	0.240230	0.000294	0.731209
1.334336	-1.149918	0.245235	0.000326	0.731203
1.543519	-1.187894	0.250240	0.000287	0.731203
1.309206	-1.284519	0.255245	0.000329	0.730936
0.637171	-1.177116	0.260250	0.000454	0.730914
0.658470	-1.176950	0.265254	0.000449	0.730923
0.681880	-1.227953	0.270259	0.000444	0.730833
0.254592	-1.279181	0.275264	0.000523	0.730588
-0.111886	-1.213069	0.280269	0.000590	0.730591
-0.002879	-1.237847	0.285274	0.000569	0.730582
0.307424	-1.349133	0.290278	0.000511	0.730475
-0.280676	-1.348838	0.295283	0.000619	0.730274
-0.396995	-1.327604	0.300288	0.000640	0.730276
-0.453267	-1.315046	0.305293	0.000650	0.730283
-0.675531	-1.359762	0.310298	0.000690	0.730121
-1.501620	-1.294991	0.315302	0.000843	0.729963
-2.133854	-1.185644	0.320307	0.000960	0.729958
-1.678854	-1.266042	0.325312	0.000875	0.729960
-1.794529	-1.245446	0.330317	0.000896	0.729962
-2.060054	-1.304604	0.335322	0.000944	0.729757
-2.630338	-1.256344	0.340326	0.001050	0.729655
-2.589810	-1.267243	0.345331	0.001041	0.729649
-2.782165	-1.235250	0.350336	0.001076	0.729646
-2.760468	-1.237373	0.355341	0.001071	0.729651
-2.804171	-1.269600	0.360346	0.001079	0.729575
-3.393556	-1.295319	0.365350	0.001188	0.729322
-3.758238	-1.234142	0.370355	0.001255	0.729317
-3.563284	-1.269350	0.375360	0.001218	0.729317
-3.378102	-1.299887	0.380365	0.001183	0.729323
-4.080604	-1.180756	0.385370	0.001312	0.729313
-3.895057	-1.248945	0.390374	0.001277	0.729246
-4.324394	-1.296902	0.395379	0.001356	0.729006
-4.424609	-1.278214	0.400384	0.001374	0.729009
-4.466340	-1.270416	0.405389	0.001381	0.729011
-4.679701	-1.237050	0.410394	0.001420	0.729004
-4.627265	-1.241797	0.415398	0.001410	0.729014
-4.834012	-1.207962	0.420403	0.001447	0.729010
-5.102061	-1.315277	0.425408	0.001496	0.728710
-5.309591	-1.284310	0.430413	0.001534	0.728700
-5.761011	-1.207530	0.435418	0.001618	0.728694
-5.312302	-1.285013	0.440422	0.001533	0.728700
-5.047796	-1.335811	0.445427	0.001483	0.728695
-5.200441	-1.311162	0.450432	0.001511	0.728691
-5.398914	-1.377124	0.455437	0.001547	0.728496
-6.499634	-1.234834	0.460442	0.001751	0.728393
-6.180467	-1.287620	0.465446	0.001691	0.728402
-6.270695	-1.276084	0.470451	0.001707	0.728395
-6.094830	-1.307536	0.475456	0.001673	0.728396
-5.979850	-1.326788	0.480461	0.001651	0.728400
-6.452417	-1.297171	0.485466	0.001738	0.728295
-7.555552	-1.212241	0.490470	0.001943	0.728080
-7.034776	-1.310094	0.495475	0.001845	0.728071
-7.337414	-1.257944	0.500480	0.001901	0.728069
-7.378846	-1.248677	0.505485	0.001908	0.728074
-7.296975	-1.265926	0.510490	0.001892	0.728071
-7.141866	-1.292442	0.515494	0.001862	0.728074
-7.298770	-1.285872	0.520499	0.001891	0.728034
-8.101172	-1.284958	0.525504	0.002039	0.727759
-7.883494	-1.322131	0.530509	0.001998	0.727764
-8.216406	-1.266795	0.535514	0.002059	0.727758
-8.192697	-1.267561	0.540518	0.002054	0.727766
-8.137102	-1.280212	0.545523	0.002043	0.727762
-8.300302	-1.252719	0.550528	0.002072	0.727760
-8.072649	-1.301084	0.555533	0.002029	0.727747
-8.731704	-1.340241	0.560538	0.002151	0.727443
-8.973883	-1.295565	0.565542	0.002195	0.727448
-9.477594	-1.209665	0.570547	0.002288	0.727442
-9.257479	-1.250718	0.575552	0.002247	0.727440
-8.834133	-1.322939	0.580557	0.002167	0.727447
-9.256484	-1.254885	0.585562	0.002245	0.727435
-9.301330	-1.241408	0.590566	0.002252	0.727447
-9.287514	-1.346133	0.595571	0.002249	0.727249
-10.087054	-1.259821	0.600576	0.002397	0.727141
-10.078821	-1.260839	0.605581	0.002395	0.727144
-10.378964	-1.210610	0.610586	0.002450	0.727139
-9.903318	-1.292303	0.615590	0.002361	0.727146
-10.302745	-1.223761	0.620595	0.002434	0.727143
-10.340270	-1.217274	0.625600	0.002440	0.727144
-10.055834	-1.294035	0.630605	0.002387	0.727094
-11.124689	-1.246452	0.635610	0.002585	0.726818
-11.400399	-1.192406	0.640614	0.002635	0.726829
-11.357813	-1.204621	0.645619	0.002627	0.726821
-11.239614	-1.227734	0.650624	0.002604	0.726819
-11.082683	-1.253620	0.655629	0.002574	0.726824
-11.268302	-1.227215	0.660634	0.002608	0.726813
-10.734772	-1.316094	0.665638	0.002507	0.726826
-11.115642	-1.293025	0.670643	0.002578	0.726740
-12.357252	-1.188256	0.675648	0.002808	0.726515
-11.691292	-1.304713	0.680653	0.002683	0.726520
-12.177726	-1.223198	0.685658	0.002773	0.726512
-12.384218	-1.182755	0.690662	0.002811	0.726521
-12.201608	-1.219453	0.695667	0.002776	0.726514
-12.231844	-1.217544	0.700672	0.002781	0.726509
-11.947708	-1.264675	0.705677	0.002727	0.726517
-12.354867	-1.262419	0.710682	0.002802	0.726381
-13.052789	-1.226461	0.715686	0.002931	0.726210
-12.758200	-1.282971	0.720691	0.002876	0.726204
-13.219500	-1.200490	0.725696	0.002961	0.726206
-12.995863	-1.239213	0.730701	0.002918	0.726210
-13.079246	-1.229561	0.735706	0.002933	0.726201
-13.245400	-1.194621	0.740710	0.002963	0.726213
-13.144503	-1.218132	0.745715	0.002943	0.726204
-13.333949	-1.297683	0.750720	0.002978	0.725984
-13.893600	-1.220992	0.755725	0.003081	0.725941
-14.296653	-1.152315	0.760730	0.003156	0.725936
-13.887043	-1.224904	0.765734	0.003079	0.725938
-14.039494	-1.199638	0.770739	0.003106	0.725936
-14.358623	-1.143942	0.775744	0.003165	0.725935
-13.729499	-1.255248	0.780749	0.003047	0.725938
-13.909246	-1.271197	0.785754	0.003080	0.725846
-14.939966	-1.211315	0.790758	0.003271	0.725606
-14.744931	-1.248945	0.795763	0.003234	0.725602
-15.126098	-1.182283	0.800768	0.003304	0.725601
-14.918242	-1.216164	0.805773	0.003264	0.725608
-15.325027	-1.149575	0.810778	0.003339	0.725598
-15.017112	-1.199071	0.815782	0.003281	0.725610
-14.830423	-1.235135	0.820787	0.003246	0.725606
-15.301242	-1.250442	0.825792	0.003332	0.725414
-16.165066	-1.168969	0.830797	0.003492	0.725274
-16.072668	-1.189365	0.835802	0.003475	0.725268
-15.954441	-1.205176	0.840806	0.003452	0.725280
-16.229819	-1.162815	0.845811	0.003502	0.725268
-16.029419	-1.197088	0.850816	0.003464	0.725272
-15.989847	-1.200614	0.855821	0.003456	0.725281
-16.321709	-1.150313	0.860826	0.003517	0.725265
-15.821779	-1.311282	0.865830	0.003423	0.725126
-17.149294	-1.176440	0.870835	0.003669	0.724929
-17.243741	-1.164729	0.875840	0.003686	0.724920
-16.827728	-1.230843	0.880845	0.003608	0.724937
-16.805496	-1.239904	0.885850	0.003603	0.724929
-16.946547	-1.210957	0.890854	0.003629	0.724938
-17.336570	-1.151575	0.895859	0.003700	0.724919
-17.141034	-1.182709	0.900864	0.003663	0.724928
-16.789983	-1.341597	0.905869	0.003597	0.724741
-18.277074	-1.148131	0.910874	0.003873	0.724603
-18.053849	-1.182243	0.915878	0.003831	0.724616
-17.726775	-1.239470	0.920883	0.003769	0.724619
-18.352393	-1.134907	0.925888	0.003885	0.724607
-18.135104	-1.169598	0.930893	0.003844	0.724616
-18.127048	-1.176771	0.935898	0.003841	0.724607
-17.834000	-1.220721	0.940902	0.003786	0.724624
-18.091900	-1.321636	0.945907	0.003833	0.724338
-19.026596	-1.193539	0.950912	0.004006	0.724265
-19.081249	-1.181493	0.955917	0.004016	0.724271
-19.115240	-1.180699	0.960922	0.004021	0.724262
-19.240687	-1.156368	0.965926	0.004044	0.724267
-19.100145	-1.182700	0.970931	0.004017	0.724266
-19.567454	-1.103964	0.975936	0.004103	0.724259
-19.450545	-1.120508	0.980941	0.004081	0.724269
-19.331088	-1.203479	0.985946	0.004058	0.724150
-19.980034	-1.186497	0.990950	0.004178	0.723958
-20.178953	-1.155741	0.995955	0.004214	0.723950
-20.407880	-1.115657	1.000960	0.004256	0.723950
-19.886565	-1.206474	1.005965	0.004158	0.723956
-20.199503	-1.157211	1.010970	0.004215	0.723945
-20.425373	-1.113726	1.015974	0.004257	0.723953
-20.128819	-1.169189	1.020979	0.004201	0.723949
-20.322193	-1.144680	1.025984	0.004236	0.723931
-20.794096	-1.213875	1.030989	0.004323	0.723632
-20.892325	-1.201083	1.035994	0.004340	0.723624
-20.980380	-1.180702	1.040998	0.004356	0.723635
-21.036354	-1.175632	1.046003	0.004366	0.723627
-21.291161	-1.131776	1.051008	0.004412	0.723626
-21.255248	-1.134064	1.056013	0.004405	0.723635
-21.298531	-1.131134	1.061018	0.004412	0.723627
-21.181180	-1.157719	1.066022	0.004389	0.723618
-21.549937	-1.236370	1.071027	0.004457	0.723336
-22.070769	-1.146621	1.076032	0.004554	0.723332
-22.213364	-1.117448	1.081037	0.004579	0.723341
-22.090152	-1.145552	1.086042	0.004556	0.723330
-21.982331	-1.160964	1.091046	0.004535	0.723339
-22.312345	-1.104592	1.096051	0.004595	0.723336
-21.965066	-1.169247	1.101056	0.004530	0.723332
-21.350597	-1.346083	1.106061	0.004415	0.723201
-23.204739	-1.122893	1.111066	0.004759	0.722993
-23.229096	-1.113779	1.116070	0.004763	0.723004
-23.126342	-1.134339	1.121075	0.004743	0.723001
-23.178411	-1.125822	1.126080	0.004752	0.723001
-23.032195	-1.150022	1.131085	0.004724	0.723006
-23.278733	-1.110978	1.136090	0.004769	0.722998
-23.075219	-1.144147	1.141094	0.004730	0.723005
-23.047120	-1.221285	1.146099	0.004724	0.722865
-24.361537	-1.081525	1.151104	0.004968	0.722682
-23.708841	-1.193680	1.156109	0.004846	0.722691
-24.098882	-1.128843	1.161114	0.004918	0.722684
-23.963112	-1.148441	1.166118	0.004892	0.722694
-23.706753	-1.198499	1.171123	0.004843	0.722687
-24.028609	-1.142462	1.176128	0.004902	0.722686
-24.269155	-1.095572	1.181133	0.004946	0.722695
-24.128473	-1.242310	1.186138	0.004919	0.722458
-24.954807	-1.141334	1.191142	0.005072	0.722369
-25.126687	-1.113391	1.196147	0.005104	0.722365
-25.321448	-1.080817	1.201152	0.005139	0.722362
-25.045244	-1.126894	1.206157	0.005087	0.722370
-24.989298	-1.141625	1.211162	0.005076	0.722362
-25.316935	-1.079468	1.216166	0.005136	0.722371
-25.361702	-1.074635	1.221171	0.005143	0.722366
-25.030123	-1.228797	1.226176	0.005081	0.722181
-25.914184	-1.125349	1.231181	0.005245	0.722077
-25.999184	-1.116809	1.236186	0.005260	0.722065
-25.627215	-1.178947	1.241190	0.005190	0.722075
-25.866226	-1.140401	1.246195	0.005233	0.722068
-26.101227	-1.100382	1.251200	0.005276	0.722066
-25.602076	-1.185644	1.256205	0.005183	0.722075
-25.769447	-1.217470	1.261210	0.005213	0.721955
-26.784697	-1.144467	1.266214	0.005401	0.721745
-26.362394	-1.222682	1.271219	0.005322	0.721740
-26.882774	-1.132045	1.276224	0.005418	0.721738
-27.092892	-1.092285	1.281229	0.005456	0.721744
-27.066932	-1.101792	1.286234	0.005451	0.721736
-26.842539	-1.140238	1.291238	0.005408	0.721740
-26.882880	-1.134880	1.296243	0.005415	0.721738
-27.574243	-1.144369	1.301248	0.005543	0.721479
-27.857630	-1.116378	1.306253	0.005595	0.721436
-27.863168	-1.119916	1.311258	0.005595	0.721429
-27.930288	-1.104708	1.316262	0.005607	0.721437
-28.152606	-1.067541	1.321267	0.005647	0.721434
-28.169895	-1.066883	1.326272	0.005650	0.721430
-27.742770	-1.139922	1.331277	0.005569	0.721438
-28.094378	-1.082591	1.336282	0.005634	0.721429
-27.997795	-1.204110	1.341286	0.005615	0.721225
-28.827102	-1.111557	1.346291	0.005769	0.721118
-29.200367	-1.046636	1.351296	0.005838	0.721117
-28.517777	-1.165250	1.356301	0.005710	0.721124
-28.809189	-1.118793	1.361306	0.005763	0.721115
-29.066739	-1.073446	1.366310	0.005810	0.721115
-29.219608	-1.045668	1.371315	0.005838	0.721118
-28.889143	-1.108006	1.376320	0.005776	0.721112
-29.123857	-1.166039	1.381325	0.005819	0.720917
-29.794659	-1.073243	1.386330	0.005943	0.720867
-29.694843	-1.087170	1.391334	0.005923	0.720876
-29.598967	-1.105591	1.396339	0.005905	0.720874
-29.888556	-1.056124	1.401344	0.005958	0.720872
-29.500085	-1.123040	1.406349	0.005885	0.720878
-29.415868	-1.143234	1.411354	0.005868	0.720869
-30.135724	-1.131771	1.416358	0.006002	0.720641
-30.992439	-1.032382	1.421363	0.006160	0.720538
-30.394097	-1.142226	1.426368	0.006048	0.720533
-30.345246	-1.148665	1.431373	0.006038	0.720538
-31.070799	-1.023384	1.436378	0.006173	0.720532
-30.881593	-1.055531	1.441382	0.006137	0.720537
-30.336442	-1.155269	1.446387	0.006034	0.720533
-30.779451	-1.098700	1.451392	0.006116	0.720491
-31.378262	-1.129731	1.456397	0.006227	0.720221
-31.482200	-1.115581	1.461402	0.006245	0.720214
-31.644728	-1.082634	1.466406	0.006275	0.720223
-31.553671	-1.100713	1.471411	0.006257	0.720221
-31.520453	-1.110513	1.476416	0.006250	0.720215
-31.490810	-1.112067	1.481421	0.006244	0.720224
-31.703662	-1.080147	1.486426	0.006283	0.720213
-31.812201	-1.188646	1.491430	0.006302	0.719963
-32.345909	-1.127986	1.496435	0.006401	0.719897
-32.731263	-1.062607	1.501440	0.006471	0.719892
-32.360735	-1.124673	1.506445	0.006402	0.719901
-32.288170	-1.144807	1.511450	0.006387	0.719888
-32.341227	-1.131912	1.516454	0.006397	0.719897
-32.568999	-1.092300	1.521459	0.006438	0.719896
-32.893046	-1.125848	1.526464	0.006498	0.719718
-33.274709	-1.117515	1.531469	0.006568	0.719602
-33.447586	-1.091004	1.536474	0.006599	0.719595
-33.321218	-1.109868	1.541478	0.006575	0.719604
-33.262901	-1.122512	1.546483	0.006563	0.719601
-33.419815	-1.097458	1.551488	0.006592	0.719596
-33.437040	-1.090947	1.556493	0.006594	0.719605
-33.779126	-1.061305	1.561498	0.006657	0.719544
-34.381428	-1.094208	1.566502	0.006769	0.719270
-34.432795	-1.086922	1.571507	0.006777	0.719267
-34.609300	-1.059644	1.576512	0.006809	0.719261
-34.053284	-1.153762	1.581517	0.006705	0.719272
-34.546859	-1.071638	1.586522	0.006796	0.719262
-34.503906	-1.075569	1.591526	0.006787	0.719271
-34.131498	-1.143439	1.596531	0.006717	0.719269
-34.759429	-1.109763	1.601536	0.006833	0.719117
-35.727488	-1.015650	1.606541	0.007013	0.718964
-35.069246	-1.136960	1.611546	0.006890	0.718957
-34.952977	-1.156799	1.616550	0.006867	0.718960
-35.506748	-1.061022	1.621555	0.006969	0.718956
-35.591345	-1.046155	1.626560	0.006984	0.718957
-34.895664	-1.168752	1.631565	0.006854	0.718961
-35.413536	-1.082494	1.636570	0.006950	0.718951
-36.143897	-1.108480	1.641574	0.007085	0.718644
-36.068270	-1.122189	1.646579	0.007070	0.718645
-36.448638	-1.058874	1.651584	0.007140	0.718638
-36.202421	-1.099526	1.656589	0.007093	0.718646
-36.445124	-1.061403	1.661594	0.007138	0.718637
-36.372419	-1.071151	1.666598	0.007123	0.718645
-36.173110	-1.108905	1.671603	0.007086	0.718642
-36.304254	-1.143986	1.676608	0.007109	0.718528
-37.081360	-1.092782	1.681613	0.007253	0.718358
-37.077075	-1.098923	1.686618	0.007252	0.718349
-37.163399	-1.080665	1.691622	0.007267	0.718356
-36.816989	-1.143197	1.696627	0.007202	0.718356
-36.942387	-1.123513	1.701632	0.007224	0.718352
-37.146192	-1.085516	1.706637	0.007261	0.718357
-37.097031	-1.159168	1.711642	0.007251	0.718230
-37.920645	-1.120420	1.716646	0.007404	0.718018
-38.019464	-1.104679	1.721651	0.007422	0.718016
-38.366431	-1.046754	1.726656	0.007485	0.718010
-37.500814	-1.197458	1.731661	0.007323	0.718018
-37.575443	-1.189225	1.736666	0.007337	0.718010
-38.138645	-1.087018	1.741670	0.007441	0.718015
-38.101816	-1.150542	1.746675	0.007433	0.717904
-38.872285	-1.116309	1.751680	0.007576	0.717702
-38.585822	-1.164769	1.756685	0.007522	0.717708
-39.357398	-1.032041	1.761690	0.007664	0.717701
-38.953451	-1.103599	1.766694	0.007588	0.717703
-38.592512	-1.169392	1.771699	0.007520	0.717701
-39.231549	-1.057665	1.776704	0.007639	0.717699
-39.016394	-1.093227	1.781709	0.007598	0.717706
-39.804885	-1.121392	1.786714	0.007744	0.717374
-40.210841	-1.045456	1.791718	0.007818	0.717382
-40.076450	-1.070779	1.796723	0.007793	0.717381
-39.770650	-1.129475	1.801728	0.007735	0.717374
-39.868738	-1.108297	1.806733	0.007752	0.717383
-40.199870	-1.054568	1.811738	0.007813	0.717374
-39.675167	-1.147835	1.816742	0.007715	0.717376
-39.855492	-1.150962	1.821747	0.007748	0.717308
-41.223232	-1.025119	1.826752	0.008001	0.717076
-40.584472	-1.133181	1.831757	0.007882	0.717089
-40.910485	-1.082255	1.836762	0.007942	0.717077
-40.914477	-1.080365	1.841766	0.007942	0.717080
-40.760308	-1.108737	1.846771	0.007912	0.717080
-40.693718	-1.121747	1.851776	0.007899	0.717079
-40.698262	-1.117509	1.856781	0.007899	0.717088
-41.306923	-1.161619	1.861786	0.008012	0.716787
-41.932067	-1.069195	1.866790	0.008127	0.716751
-41.816035	-1.090499	1.871795	0.008105	0.716751
-41.950566	-1.069931	1.876800	0.008129	0.716746
-41.829418	-1.085797	1.881805	0.008106	0.716759
-41.838112	-1.091351	1.886810	0.008107	0.716746
-41.803406	-1.094935	1.891814	0.008099	0.716753
-41.560795	-1.180187	1.896819	0.008053	0.716671
-42.588303	-1.113846	1.901824	0.008244	0.716442
-42.438438	-1.138221	1.906829	0.008215	0.716448
-43.122004	-1.020520	1.911834	0.008342	0.716441
-42.678984	-1.096958	1.916838	0.008258	0.716448
-42.357911	-1.155496	1.921843	0.008198	0.716447
-43.320768	-0.988044	1.926848	0.008376	0.716440
-42.616379	-1.108912	1.931853	0.008244	0.716451
-42.719753	-1.239340	1.936858	0.008263	0.716157
-43.600037	-1.095850	1.941862	0.008426	0.716132
-44.001436	-1.026046	1.946867	0.008500	0.716131
-43.575262	-1.106420	1.951872	0.008420	0.716123
-43.258697	-1.160689	1.956877	0.008360	0.716129
-43.803373	-1.066110	1.961882	0.008461	0.716126
-43.654127	-1.090614	1.966886	0.008432	0.716131
-43.580429	-1.191865	1.971891	0.008418	0.715958
-44.759534	-1.021524	1.976896	0.008636	0.715881
-44.258251	-1.107835	1.981901	0.008542	0.715888
-44.300261	-1.105476	1.986906	0.008549	0.715880
-44.504737	-1.066772	1.991910	0.008587	0.715886
-44.313808	-1.101616	1.996915	0.008550	0.715886
-44.433696	-1.133463	2.001920	0.008572	0.715782

-45.474249	-1.068293	2.011917	0.008764	0.715546
-45.306760	-1.100857	2.021914	0.008731	0.715544
-45.255871	-1.110009	2.031910	0.008720	0.715547
-45.433384	-1.079655	2.041907	0.008752	0.715547
-45.173725	-1.128757	2.051904	0.008702	0.715544
-45.657610	-1.045441	2.061901	0.008790	0.715542
-45.325277	-1.105795	2.071898	0.008727	0.715542
-45.246818	-1.120844	2.081894	0.008711	0.715543
-45.260055	-1.118651	2.091891	0.008711	0.715546
-44.739233	-1.112538	2.101888	0.008613	0.715745
-44.707892	-1.049564	2.111885	0.008605	0.715884
-44.307255	-1.122635	2.121882	0.008529	0.715883
-44.370753	-1.113578	2.131878	0.008540	0.715882
-44.511417	-1.090184	2.141875	0.008564	0.715882
-44.452048	-1.101516	2.151872	0.008552	0.715883
-44.744284	-1.032192	2.161869	0.008604	0.715920
-43.954538	-1.070891	2.171866	0.008456	0.716125
-43.837073	-1.092730	2.181862	0.008432	0.716127
-43.791405	-1.101739	2.191859	0.008422	0.716128
-43.703581	-1.097114	2.201856	0.008404	0.716171
-43.169794	-1.057739	2.211853	0.008303	0.716440
-42.869031	-1.111636	2.221850	0.008246	0.716443
-43.215069	-1.050672	2.231846	0.008309	0.716444
-42.721033	-1.077467	2.241843	0.008215	0.716568
-42.133722	-1.092675	2.251840	0.008104	0.716748
-42.220122	-1.079185	2.261837	0.008119	0.716748
-42.101378	-1.102395	2.271834	0.008095	0.716747
-41.370738	-1.110012	2.281830	0.007957	0.716992
-41.158935	-1.105362	2.291827	0.007916	0.717079
-41.085919	-1.118569	2.301824	0.007901	0.717081
-41.215866	-1.096770	2.311821	0.007924	0.717082
-40.603091	-1.065586	2.321818	0.007808	0.717362
-40.540966	-1.073099	2.331814	0.007795	0.717372
-40.251956	-1.123080	2.341811	0.007740	0.717378
-40.363968	-1.008709	2.351808	0.007759	0.717568
-39.509902	-1.096082	2.361805	0.007598	0.717699
-39.576138	-1.086619	2.371802	0.007609	0.717697
-39.631004	-1.050478	2.381798	0.007618	0.717752
-38.694111	-1.087758	2.391795	0.007442	0.718011
-38.757217	-1.077074	2.401792	0.007452	0.718013
-38.808667	-1.069217	2.411789	0.007460	0.718014
-37.984849	-1.086423	2.421786	0.007305	0.718272
-37.990828	-1.049270	2.431782	0.007304	0.718347
-37.548069	-1.128169	2.441779	0.007220	0.718350
-37.934907	-1.034854	2.451776	0.007291	0.718401
-36.873526	-1.105180	2.461773	0.007092	0.718638
-36.969840	-1.091432	2.471770	0.007108	0.718634
-36.873906	-1.107371	2.481766	0.007089	0.718640
-36.478673	-1.073821	2.491763	0.007013	0.718848
-36.023013	-1.100753	2.501760	0.006927	0.718958
-36.138382	-1.082305	2.511757	0.006947	0.718957
-36.012459	-1.078391	2.521754	0.006922	0.719011
-35.405576	-1.059375	2.531750	0.006807	0.719265
-35.226696	-1.090716	2.541747	0.006772	0.719269
-35.447513	-1.053410	2.551744	0.006812	0.719268
-34.658397	-1.048008	2.561741	0.006663	0.719559
-34.642321	-1.033743	2.571738	0.006659	0.719596
-34.277391	-1.098177	2.581734	0.006589	0.719600
-34.096235	-1.056648	2.591731	0.006554	0.719748
-33.402648	-1.105448	2.601728	0.006423	0.719898
-33.560858	-1.078539	2.611725	0.006451	0.719899
-33.687074	-1.047730	2.621722	0.006473	0.719918
-32.838359	-1.046367	2.631718	0.006314	0.720221
-32.808197	-1.052052	2.641715	0.006306	0.720224
-32.784330	-1.056538	2.651712	0.006300	0.720226
-32.273429	-1.026067	2.661709	0.006204	0.720468
-32.131457	-1.017801	2.671706	0.006176	0.720537
-31.631123	-1.106540	2.681702	0.006081	0.720541
-31.683547	-1.042130	2.691699	0.006089	0.720652
-31.014564	-1.048113	2.701696	0.005963	0.720878
-30.830507	-1.082831	2.711693	0.005927	0.720877
-30.976839	-1.060184	2.721690	0.005953	0.720873
-30.424501	-1.061526	2.731686	0.005848	0.721067
-30.214316	-1.073878	2.741683	0.005808	0.721120
-30.115647	-1.091205	2.751680	0.005788	0.721123
-30.096887	-1.021501	2.761677	0.005783	0.721270
-29.511803	-1.044357	2.771674	0.005672	0.721432
-29.282097	-1.087203	2.781670	0.005628	0.721432
-29.237362	-1.067613	2.791667	0.005618	0.721489
-28.380997	-1.091344	2.801664	0.005457	0.721745
-28.147818	-1.136040	2.811661	0.005412	0.721741
-28.283545	-1.114530	2.821658	0.005436	0.721739
-27.953505	-1.110966	2.831654	0.005373	0.721865
-27.217470	-1.138303	2.841651	0.005234	0.722071
-27.268807	-1.128557	2.851648	0.005242	0.722076
-27.487371	-1.090786	2.861645	0.005281	0.722076
-26.754803	-1.111621	2.871642	0.005143	0.722294
-26.365974	-1.144665	2.881638	0.005069	0.722368
-26.748686	-1.077547	2.891635	0.005139	0.722369
-26.423035	-1.104950	2.901632	0.005077	0.722432
-25.483507	-1.142582	2.911629	0.004900	0.722690
-25.695920	-1.105628	2.921626	0.004938	0.722691
-25.474282	-1.145003	2.931622	0.004895	0.722694
-25.374800	-1.078864	2.941619	0.004875	0.722862
-24.563450	-1.151963	2.951616	0.004722	0.723005
-24.996223	-1.076373	2.961613	0.004801	0.723005
-24.777671	-1.099737	2.971610	0.004759	0.723038
-24.067488	-1.075923	2.981606	0.004625	0.723336
-23.706220	-1.138601	2.991603	0.004557	0.723342
-23.673588	-1.146433	3.001600	0.004549	0.723341
-23.660937	-1.065112	3.011597	0.004545	0.723508
-23.097327	-1.104557	3.021594	0.004438	0.723630
-22.946466	-1.130488	3.031590	0.004409	0.723635
-23.037679	-1.091665	3.041587	0.004424	0.723682
-22.099360	-1.119093	3.051584	0.004248	0.723958
-22.269900	-1.090035	3.061581	0.004278	0.723959
-21.890874	-1.160337	3.071578	0.004206	0.723956
-21.614421	-1.125786	3.081574	0.004153	0.724123
-20.798060	-1.196077	3.091571	0.003999	0.724273
-20.892721	-1.181168	3.101568	0.004015	0.724272
-21.131279	-1.142596	3.111565	0.004058	0.724268
-20.659721	-1.112874	3.121562	0.003969	0.724493
-20.087242	-1.154001	3.131558	0.003861	0.724615
-20.208358	-1.133104	3.141555	0.003882	0.724617
-19.970737	-1.176752	3.151552	0.003836	0.724617
-19.746060	-1.073494	3.161549	0.003792	0.724900
-19.185355	-1.160354	3.171546	0.003686	0.724928
-19.472750	-1.115410	3.181542	0.003738	0.724919
-18.967560	-1.111826	3.191539	0.003643	0.725105
-18.119150	-1.176830	3.201536	0.003483	0.725276
-18.429786	-1.127232	3.211533	0.003539	0.725268
-18.283051	-1.152220	3.221530	0.003511	0.725273
-17.823050	-1.102391	3.231526	0.003423	0.725533
-17.598767	-1.107269	3.241523	0.003380	0.725605
-17.190221	-1.180421	3.251520	0.003302	0.725607
-17.514757	-1.101195	3.261517	0.003361	0.725652
-16.402733	-1.155236	3.271514	0.003153	0.725936
-16.544779	-1.130094	3.281510	0.003177	0.725939
-16.356873	-1.163208	3.291507	0.003141	0.725942
-16.318346	-1.112785	3.301504	0.003132	0.726057
-15.557488	-1.170840	3.311501	0.002989	0.726211
-15.489784	-1.185196	3.321498	0.002975	0.726209
-15.884631	-1.114133	3.331494	0.003047	0.726214
-15.069732	-1.124728	3.341491	0.002893	0.726479
-14.885789	-1.138992	3.351488	0.002858	0.726518
-14.734913	-1.167593	3.361485	0.002828	0.726518
-14.711082	-1.105413	3.371482	0.002822	0.726650
-14.145285	-1.120861	3.381478	0.002715	0.726820
-13.996278	-1.146725	3.391475	0.002686	0.726824
-14.110642	-1.107639	3.401472	0.002705	0.726863
-13.119229	-1.141142	3.411469	0.002519	0.727145
-13.058350	-1.152881	3.421466	0.002506	0.727146
-13.116209	-1.143686	3.431462	0.002515	0.727147
-12.694648	-1.133154	3.441459	0.002435	0.727317
-12.106597	-1.171803	3.451456	0.002324	0.727448
-11.895260	-1.211405	3.461453	0.002283	0.727447
-12.201763	-1.159557	3.471450	0.002339	0.727445
-11.361387	-1.161634	3.481446	0.002181	0.727735
-11.041967	-1.204585	3.491443	0.002120	0.727765
-11.154732	-1.185296	3.501440	0.002139	0.727767
-10.893857	-1.224848	3.511437	0.002089	0.727783
-10.354439	-1.174485	3.521434	0.001987	0.728071
-10.255607	-1.193419	3.531430	0.001967	0.728071
-10.213600	-1.199189	3.541427	0.001958	0.728078
-10.196465	-1.125024	3.551424	0.001953	0.728231
-9.127487	-1.231264	3.561421	0.001752	0.728397
-9.277095	-1.205338	3.571418	0.001779	0.728399
-9.177956	-1.223683	3.581414	0.001759	0.728401
-9.012448	-1.142791	3.591411	0.001726	0.728618
-8.656373	-1.165247	3.601408	0.001658	0.728701
-8.518037	-1.191814	3.611405	0.001631	0.728700
-8.507197	-1.129597	3.621402	0.001627	0.728828
-7.614177	-1.196160	3.631398	0.001460	0.729010
-7.572204	-1.204250	3.641395	0.001450	0.729012
-7.607488	-1.197424	3.651392	0.001455	0.729016
-7.164960	-1.145268	3.661389	0.001371	0.729273
-6.870550	-1.177094	3.671386	0.001315	0.729316
-6.865741	-1.177041	3.681382	0.001312	0.729321
-6.831868	-1.095377	3.691379	0.001304	0.729494
-6.422539	-1.088435	3.701376	0.001227	0.729652
-5.936673	-1.176969	3.711373	0.001135	0.729651
-5.944201	-1.130223	3.721370	0.001134	0.729742
-5.344118	-1.130153	3.731366	0.001021	0.729953
-5.217780	-1.151564	3.741363	0.000996	0.729958
-5.500161	-1.088487	3.751360	0.001047	0.729985
-4.746552	-1.073947	3.761357	0.000905	0.730277
-4.556062	-1.107497	3.771354	0.000868	0.730281
-4.898976	-1.039884	3.781350	0.000930	0.730296
-3.925058	-1.058517	3.791347	0.000747	0.730599
-4.086749	-1.031046	3.801344	0.000776	0.730600
-3.786340	-1.088828	3.811341	0.000718	0.730594
-3.957938	-0.895446	3.821338	0.000749	0.730913
-3.020154	-1.060038	3.831334	0.000573	0.730920
-2.921038	-1.078575	3.841331	0.000553	0.730922
-2.813173	-0.950650	3.851328	0.000531	0.731210
-2.844664	-0.945865	3.861325	0.000535	0.731211
-3.049120	-0.859699	3.871322	0.000572	0.731310
-2.855907	-0.788187	3.881318	0.000534	0.731519
-2.360203	-0.876888	3.891315	0.000440	0.731520
-2.199906	-0.749896	3.901312	0.000409	0.731825
-1.550731	-0.865701	3.911309	0.000286	0.731827
-1.413464	-0.821933	3.921306	0.000259	0.731962
-1.556264	-0.703047	3.931302	0.000284	0.732146
-1.747734	-0.637740	3.941299	0.000318	0.732209
-1.578642	-0.546047	3.951296	0.000285	0.732448
-1.268746	-0.570419	3.961293	0.000226	0.732510
-0.955718	-0.497213	3.971290	0.000166	0.732763
-0.876311	-0.478539	3.981286	0.000149	0.732829
-0.342707	-0.446418	3.991283	0.000048	0.733077
-0.223202	-0.443393	4.001280	0.000025	0.733127
-0.351580	-0.275968	4.011277	0.000047	0.733410
-0.695939	-0.158004	4.021274	0.000109	0.733522
-0.231721	-0.144000	4.031270	0.000021	0.733712
-0.237395	-0.028360	4.041267	0.000021	0.733936
-0.061526	0.005024	4.051264	-0.000014	0.734064
0.000000	0.185918	4.061261	-0.000027	0.734437

0.109304	0.808926	4.066266	-0.000048	0.735677
0.380140	2.034509	4.071270	-0.000100	0.738128
1.423714	3.744244	4.076275	-0.000297	0.741760
2.325382	6.050733	4.081280	-0.000467	0.746459
2.927116	8.941611	4.086285	-0.000581	0.752130
3.807021	12.262193	4.091290	-0.000748	0.758654
5.140436	15.949106	4.096294	-0.001000	0.765950
6.160125	20.148195	4.101299	-0.001193	0.774012
6.600434	24.831364	4.106304	-0.001279	0.782681
7.203627	29.860891	4.111309	-0.001395	0.791927
8.134569	35.172538	4.116314	-0.001573	0.801668
8.683395	40.874272	4.121318	-0.001680	0.811854
9.300564	46.861284	4.126323	-0.001799	0.822425
9.927241	53.142595	4.131328	-0.001921	0.833366
10.303782	59.695295	4.136333	-0.001996	0.844546
11.013541	66.432061	4.141338	-0.002133	0.855982
11.780729	73.360844	4.146342	-0.002281	0.867597
12.686285	80.484879	4.151347	-0.002455	0.879411
13.422959	87.819741	4.156352	-0.002598	0.891357
14.357338	95.291215	4.161357	-0.002778	0.903413
15.495437	102.908195	4.166362	-0.002996	0.915590
15.990921	110.742289	4.171366	-0.003094	0.927766
16.534637	118.707911	4.176371	-0.003201	0.939995
17.163791	126.754264	4.181376	-0.003324	0.952209
17.749551	134.892560	4.186381	-0.003439	0.964391
18.430854	143.130353	4.191386	-0.003572	0.976590
19.066690	151.445996	4.196390	-0.003697	0.988738
19.929607	159.793941	4.201395	-0.003864	1.000840
20.594907	168.208660	4.206400	-0.003994	1.012843
21.134493	176.687159	4.211405	-0.004101	1.024762
21.993445	185.168847	4.216410	-0.004267	1.036624
22.790835	193.669045	4.221414	-0.004422	1.048362
23.657404	202.211556	4.226419	-0.004589	1.060041
24.388052	210.805793	4.231424	-0.004732	1.071631
24.926005	219.428088	4.236429	-0.004838	1.083089
25.445764	228.080050	4.241434	-0.004942	1.094461
25.975063	236.714182	4.246438	-0.005047	1.105696
26.557177	245.363465	4.251443	-0.005161	1.116847
27.128352	253.994413	4.256448	-0.005274	1.127863
27.718911	262.628078	4.261453	-0.005391	1.138780
28.337643	271.275497	4.266458	-0.005512	1.149615
28.880461	279.917073	4.271462	-0.005620	1.160326
29.469319	288.523872	4.276467	-0.005736	1.170906
29.862286	297.149244	4.281472	-0.005815	1.181373
30.190207	305.782782	4.286477	-0.005883	1.191744
30.617672	314.374123	4.291482	-0.005969	1.201996
31.350873	322.916283	4.296486	-0.006112	1.212165
31.978620	331.469583	4.301491	-0.006235	1.222240
32.335424	340.069480	4.306496	-0.006308	1.232234
32.877334	348.594380	4.311501	-0.006415	1.242098
33.414427	357.132937	4.316506	-0.006521	1.251897
33.824512	365.648772	4.321510	-0.006604	1.261571
34.263575	374.174982	4.326515	-0.006692	1.271188
34.927392	382.630414	4.331520	-0.006822	1.280697
35.014879	391.169838	4.336525	-0.006845	1.290120
35.734823	399.600009	4.341530	-0.006985	1.299472
36.341401	408.056179	4.346534	-0.007104	1.308765
36.705397	416.620678	4.351539	-0.007178	1.318064
37.102275	425.026903	4.356544	-0.007259	1.327135
37.681548	433.410005	4.361549	-0.007373	1.336152
38.272711	441.790589	4.366554	-0.007489	1.345108
38.718394	450.186223	4.371558	-0.007578	1.353994
39.234119	458.564850	4.376563	-0.007681	1.362817
39.581981	466.963114	4.381568	-0.007752	1.371575
40.123469	475.309087	4.386573	-0.007859	1.380256
40.498864	483.700273	4.391578	-0.007935	1.388900
40.909784	492.069330	4.396582	-0.008018	1.397475
41.289570	500.403724	4.401587	-0.008094	1.405957
41.790200	508.740567	4.406592	-0.008194	1.414410
42.002110	517.083569	4.411597	-0.008240	1.422771
42.536922	525.405556	4.416602	-0.008345	1.431116
42.838232	533.732285	4.421606	-0.008408	1.439379
43.312463	542.029259	4.426611	-0.008502	1.447593
43.634510	550.363010	4.431616	-0.008568	1.455772
44.320057	558.605676	4.436621	-0.008702	1.463875
44.874687	566.931750	4.441626	-0.008812	1.471992
45.307896	575.219887	4.446630	-0.008899	1.480010
45.716252	583.495992	4.451635	-0.008981	1.487968
45.983380	591.802164	4.456640	-0.009037	1.495891
46.489596	600.040141	4.461645	-0.009137	1.503745
47.028068	608.308314	4.466650	-0.009244	1.511591
47.545928	616.548327	4.471654	-0.009346	1.519366
47.656882	624.850470	4.476659	-0.009373	1.527098
48.323337	633.066924	4.481664	-0.009503	1.534796
48.629440	641.322743	4.486669	-0.009566	1.542437
48.856253	649.604932	4.491674	-0.009615	1.550052
49.176016	657.865230	4.496678	-0.009681	1.557624
49.685085	666.062906	4.501683	-0.009781	1.565131
50.198756	674.285296	4.506688	-0.009883	1.572624
50.221228	682.554632	4.511693	-0.009894	1.580053
50.956506	690.730154	4.516698	-0.010037	1.587465
51.371159	698.956798	4.521702	-0.010120	1.594843
51.532321	707.208548	4.526707	-0.010156	1.602172
51.869782	715.427265	4.531712	-0.010225	1.609464
51.992366	723.673911	4.536717	-0.010254	1.616717
52.479073	731.858853	4.541722	-0.010351	1.623935
52.706891	740.119678	4.546726	-0.010399	1.631151
53.242011	748.305087	4.551731	-0.010505	1.638312
53.754727	756.446861	4.556736	-0.010607	1.645401
53.805461	764.699208	4.561741	-0.010622	1.652491
54.465521	772.837658	4.566746	-0.010751	1.659536
54.557289	781.048790	4.571750	-0.010775	1.666536
54.815597	789.265962	4.576755	-0.010829	1.673535
55.250864	797.411408	4.581760	-0.010916	1.680467
55.524119	805.593000	4.586765	-0.010973	1.687380
55.967446	813.782534	4.591770	-0.011062	1.694293
56.107685	821.979002	4.596774	-0.011094	1.701144
56.729894	830.115952	4.601779	-0.011216	1.707981
57.085459	838.323454	4.606784	-0.011288	1.714815
57.172508	846.497895	4.611789	-0.011310	1.721559
57.556105	854.662142	4.616794	-0.011388	1.728306
58.100920	862.800328	4.621798	-0.011496	1.735027
58.208362	870.996145	4.626803	-0.011522	1.741713
58.374967	879.176738	4.631808	-0.011559	1.748368
58.511536	887.370171	4.636813	-0.011590	1.755004
59.046279	895.485622	4.641818	-0.011696	1.761603
59.240048	903.652254	4.646822	-0.011738	1.768175
59.522915	911.825059	4.651827	-0.011797	1.774739
59.917186	919.948822	4.656832	-0.011877	1.781253
60.119661	928.109453	4.661837	-0.011920	1.787749
60.469912	936.332509	4.666842	-0.011992	1.794289
60.834939	944.416974	4.671846	-0.012066	1.800698
61.427358	952.513392	4.676851	-0.012182	1.807121
61.775443	960.672161	4.681856	-0.012253	1.813540
62.024438	968.803207	4.686861	-0.012305	1.819903
62.223124	976.964890	4.691866	-0.012349	1.826262
62.329207	985.142802	4.696870	-0.012374	1.832599
62.931413	993.227659	4.701875	-0.012493	1.838902
63.212289	1001.364928	4.706880	-0.012551	1.845186
63.283324	1009.537682	4.711885	-0.012570	1.851451
63.456475	1017.706185	4.716890	-0.012609	1.857703
63.716466	1025.828040	4.721894	-0.012663	1.863909
63.976699	1033.974514	4.726899	-0.012718	1.870113
64.201835	1042.129438	4.731904	-0.012766	1.876299
64.552742	1050.215502	4.736909	-0.012837	1.882426
64.981302	1058.327490	4.741914	-0.012923	1.888563
65.175499	1066.474912	4.746918	-0.012965	1.894679
65.604083	1074.565062	4.751923	-0.013051	1.900759
66.020659	1082.670930	4.756928	-0.013135	1.906830
66.179781	1090.822359	4.761933	-0.013171	1.912886
66.548896	1098.934599	4.766938	-0.013245	1.918918
66.805581	1107.039346	4.771942	-0.013299	1.924912
66.946603	1115.191944	4.776947	-0.013332	1.930911
67.249974	1123.326369	4.781952	-0.013394	1.936895
67.462019	1131.428581	4.786957	-0.013440	1.942827
68.077824	1139.522235	4.791962	-0.013560	1.948779
68.063366	1147.710247	4.796966	-0.013564	1.954713
68.370482	1155.788888	4.801971	-0.013627	1.960584
68.805283	1163.878576	4.806976	-0.013714	1.966459
68.928867	1172.011479	4.811981	-0.013743	1.972315
69.280202	1180.128596	4.816986	-0.013815	1.978166
69.449859	1188.217656	4.821990	-0.013852	1.983960
69.792072	1196.325060	4.826995	-0.013922	1.989769
69.994681	1204.454746	4.832000	-0.013966	1.995562
70.123487	1212.555150	4.837005	-0.013996	2.001310
70.543282	1220.641388	4.842010	-0.014080	2.007061
70.901826	1228.746261	4.847014	-0.014153	2.012803
71.167875	1236.853290	4.852019	-0.014209	2.018520
71.512447	1244.952968	4.857024	-0.014279	2.024224
71.489218	1253.099989	4.862029	-0.014281	2.029907
71.715637	1261.236693	4.867034	-0.014329	2.035592
71.968966	1269.289672	4.872038	-0.014382	2.041207
72.478736	1277.345018	4.877043	-0.014483	2.046833
72.682617	1285.478226	4.882048	-0.014527	2.052467
72.725693	1293.585054	4.887053	-0.014541	2.058051
73.176715	1301.654761	4.892058	-0.014631	2.063635
73.087900	1309.784428	4.897062	-0.014621	2.069191
73.369399	1317.897466	4.902067	-0.014679	2.074758
73.791183	1325.952413	4.907072	-0.014764	2.080284
73.905478	1334.046454	4.912077	-0.014791	2.085791
74.028992	1342.182588	4.917082	-0.014820	2.091314
74.316533	1350.262632	4.922086	-0.014880	2.096800
74.763188	1358.309478	4.927091	-0.014969	2.102264
74.978157	1366.435334	4.932096	-0.015015	2.107745
75.253114	1374.581560	4.937101	-0.015072	2.113232
75.617831	1382.655329	4.942106	-0.015146	2.118664
75.614885	1390.740958	4.947110	-0.015152	2.124054
75.869288	1398.807066	4.952115	-0.015205	2.129443
76.397858	1406.874929	4.957120	-0.015310	2.134845
76.639898	1414.936488	4.962125	-0.015361	2.140203
76.669158	1423.072143	4.967130	-0.015372	2.145575
76.945057	1431.144035	4.972134	-0.015430	2.150916
77.217968	1439.229262	4.977139	-0.015487	2.156251
77.400017	1447.308574	4.982144	-0.015527	2.161561
77.593744	1455.391893	4.987149	-0.015569	2.166861
78.309489	1463.436709	4.992154	-0.015708	2.172172
78.394221	1471.552735	4.997158	-0.015730	2.177458
78.379454	1479.660519	5.002163	-0.015733	2.182716
78.560539	1487.755278	5.007168	-0.015773	2.187972
79.126493	1495.819543	5.012173	-0.015885	2.193230
79.254240	1503.921353	5.017178	-0.015914	2.198459
79.288702	1511.998566	5.022182	-0.015927	2.203652
79.652474	1520.050416	5.027187	-0.016001	2.208847
79.826973	1528.166957	5.032192	-0.016039	2.214053
80.029503	1536.216495	5.037197	-0.016083	2.219207
80.238673	1544.303619	5.042202	-0.016128	2.224373
80.537207	1552.375285	5.047206	-0.016190	2.229525
80.455919	1560.518023	5.052211	-0.016181	2.234677
80.711088	1568.565484	5.057216	-0.016234	2.239787
80.902119	1576.614450	5.062221	-0.016276	2.244880
81.182275	1584.719848	5.067226	-0.016334	2.250004
81.395703	1592.776801	5.072230	-0.016380	2.255081
81.848879	1600.839470	5.077235	-0.016470	2.260171
82.177958	1608.908112	5.082240	-0.016537	2.265242
82.310605	1617.020801	5.087245	-0.016568	2.270313
82.767087	1625.153144	5.092250	-0.016659	2.275412
82.935063	1633.179536	5.097254	-0.016697	2.280409
83.193183	1641.226114	5.102259	-0.016751	2.285415
83.643133	1649.267131	5.107264	-0.016840	2.290423
83.792703	1657.346628	5.112269	-0.016874	2.295419
84.062722	1665.425262	5.117274	-0.016931	2.300413
84.276648	1673.463430	5.122278	-0.016977	2.305366
84.690754	1681.520956	5.127283	-0.017060	2.310338
84.854306	1689.640131	5.132288	-0.017096	2.315316
84.970097	1697.695822	5.137293	-0.017124	2.320240
85.382402	1705.740077	5.142298	-0.017207	2.325171
85.707897	1713.803757	5.147302	-0.017273	2.330096
85.902463	1721.894038	5.152307	-0.017316	2.335017
86.223738	1729.965718	5.157312	-0.017381	2.339926
86.430354	1738.019134	5.162317	-0.017426	2.344804
86.631464	1746.111233	5.167322	-0.017469	2.349695
86.835667	1754.214207	5.172326	-0.017514	2.354583
87.162564	1762.240228	5.177331	-0.017580	2.359424
87.458453	1770.289236	5.182336	-0.017642	2.364266
87.538514	1778.369896	5.187341	-0.017663	2.369100
87.694377	1786.477642	5.192346	-0.017698	2.373946
87.932039	1794.519652	5.197350	-0.017748	2.378750
87.939220	1802.603201	5.202355	-0.017755	2.383550
88.061779	1810.675225	5.207360	-0.017784	2.388344
88.634708	1818.696216	5.212365	-0.017897	2.393132
88.656380	1826.801163	5.217370	-0.017907	2.397918
88.545208	1834.866549	5.222374	-0.017892	2.402660
88.976822	1842.895502	5.227379	-0.017979	2.407413
89.241258	1850.971362	5.232384	-0.018034	2.412172
89.328332	1859.039658	5.237389	-0.018056	2.416903
89.546728	1867.103223	5.242394	-0.018103	2.421632
89.624562	1875.168887	5.247398	-0.018123	2.426343
89.655265	1883.294634	5.252403	-0.018135	2.431075
90.238738	1891.349876	5.257408	-0.018250	2.435800
90.403709	1899.370371	5.262413	-0.018287	2.440463
90.695830	1907.395811	5.267418	-0.018347	2.445130
90.860283	1915.455717	5.272422	-0.018384	2.449798
91.032062	1923.533407	5.277427	-0.018422	2.454468
91.273553	1931.589235	5.282432	-0.018473	2.459122
91.298126	1939.632537	5.287437	-0.018483	2.463744
91.736703	1947.689252	5.292442	-0.018571	2.468395
91.899321	1955.760837	5.297446	-0.018607	2.473026
92.223931	1963.807703	5.302451	-0.018674	2.477645
92.355862	1971.859489	5.307456	-0.018705	2.482245
92.477809	1979.908103	5.312461	-0.018733	2.486834
92.719376	1987.990562	5.317466	-0.018784	2.491442
92.709444	1996.083205	5.322470	-0.018789	2.496029
92.634198	2004.149749	5.327475	-0.018781	2.500587
93.124096	2012.169696	5.332480	-0.018878	2.505153
93.176177	2020.242969	5.337485	-0.018894	2.509708
93.394151	2028.348770	5.342490	-0.018940	2.514286
93.633641	2036.373544	5.347494	-0.018991	2.518811
93.886382	2044.381115	5.352499	-0.019044	2.523319
94.096940	2052.446263	5.357504	-0.019089	2.527848
94.420831	2060.485243	5.362509	-0.019155	2.532363
94.716444	2068.545752	5.367514	-0.019217	2.536879
94.731746	2076.618092	5.372518	-0.019225	2.541374
94.845541	2084.667752	5.377523	-0.019253	2.545856
94.907441	2092.746439	5.382528	-0.019270	2.550342
95.212434	2100.791634	5.387533	-0.019333	2.554818
95.427030	2108.840543	5.392538	-0.019379	2.559283
95.495935	2116.879036	5.397542	-0.019398	2.563723
95.669986	2124.940084	5.402547	-0.019436	2.568176
95.774624	2133.023706	5.407552	-0.019462	2.572629
95.883774	2141.053388	5.412557	-0.019488	2.577044
96.338324	2149.086295	5.417562	-0.019579	2.581478
96.366608	2157.143380	5.422566	-0.019590	2.585888
96.499752	2165.241447	5.427571	-0.019621	2.590320
96.937832	2173.447731	5.432576	-0.019709	2.594824
97.072406	2181.417949	5.437581	-0.019740	2.599171
97.338634	2189.430905	5.442586	-0.019795	2.603543
97.432875	2197.442333	5.447590	-0.019819	2.607895
97.655192	2205.478411	5.452595	-0.019866	2.612261
97.816006	2213.549007	5.457600	-0.019902	2.616635
97.819754	2221.580308	5.462605	-0.019909	2.620970
98.051286	2229.614713	5.467610	-0.019958	2.625315
98.327136	2237.644031	5.472614	-0.020016	2.629652
98.421290	2245.725485	5.477619	-0.020039	2.633999
98.742001	2253.748451	5.482624	-0.020105	2.638321
98.797451	2261.787619	5.487629	-0.020121	2.642628
99.097271	2269.821349	5.492634	-0.020183	2.646941
99.355462	2277.869959	5.497638	-0.020237	2.651252
99.572557	2285.949474	5.502643	-0.020284	2.655570
99.737326	2294.001663	5.507648	-0.020320	2.659863
99.767113	2302.029876	5.512653	-0.020332	2.664127
100.240855	2310.092369	5.517658	-0.020426	2.668431
100.243145	2318.165857	5.522662	-0.020433	2.672704
100.478962	2326.218607	5.527667	-0.020483	2.676974
100.649440	2334.244895	5.532672	-0.020520	2.681219
100.840796	2342.257163	5.537677	-0.020562	2.685451
101.097832	2350.306345	5.542682	-0.020616	2.689700
101.212205	2358.370744	5.547686	-0.020643	2.693941
101.494492	2366.406250	5.552691	-0.020702	2.698171
101.647834	2374.452132	5.557696	-0.020736	2.702392
101.621937	2382.510080	5.562701	-0.020738	2.706601
101.822577	2390.579174	5.567706	-0.020781	2.710824
101.908841	2398.654265	5.572710	-0.020803	2.715036
102.160506	2406.647708	5.577715	-0.020856	2.719209
102.350321	2414.684425	5.582720	-0.020897	2.723394
102.517564	2422.729684	5.587725	-0.020935	2.727576
102.750815	2430.789207	5.592730	-0.020984	2.731763
102.874726	2438.856685	5.597734	-0.021013	2.735941
102.943009	2446.889286	5.602739	-0.021032	2.740091
103.182193	2454.915722	5.607744	-0.021082	2.744242
103.278996	2462.977340	5.612749	-0.021107	2.748396
103.683631	2471.090953	5.617754	-0.021188	2.752589
103.862802	2479.122507	5.622758	-0.021227	2.756720
104.078519	2487.132038	5.627763	-0.021274	2.760836
104.275705	2495.158882	5.632768	-0.021316	2.764953
104.524922	2503.162963	5.637773	-0.021369	2.769056
104.574558	2511.264895	5.642778	-0.021384	2.773190
104.863821	2519.290854	5.647782	-0.021444	2.777294
104.988583	2527.313610	5.652787	-0.021473	2.781381
105.306889	2535.357734	5.657792	-0.021538	2.785483
105.424676	2543.389733	5.662797	-0.021566	2.789562
105.697567	2551.463729	5.667802	-0.021623	2.793665
106.084742	2559.475950	5.672806	-0.021701	2.797737
106.185071	2567.529499	5.677811	-0.021726	2.801808
106.312362	2575.581797	5.682816	-0.021756	2.805873
106.478082	2583.594243	5.687821	-0.021793	2.809915
106.760765	2591.677630	5.692826	-0.021851	2.813993
106.813069	2599.720892	5.697830	-0.021867	2.818032
107.099714	2607.735167	5.702835	-0.021926	2.822064
107.323406	2615.786382	5.707840	-0.021974	2.826105
107.490807	2623.820036	5.712845	-0.022011	2.830128
107.447109	2631.952538	5.717850	-0.022009	2.834183
107.799040	2639.925599	5.722854	-0.022081	2.838175
107.940482	2647.943419	5.727859	-0.022113	2.842172
108.132684	2655.986982	5.732864	-0.022155	2.846179
108.448159	2663.982695	5.737869	-0.022220	2.850163
108.827557	2672.046255	5.742874	-0.022296	2.854179
108.728999	2680.122888	5.747878	-0.022284	2.858169
108.815435	2688.145025	5.752883	-0.022306	2.862137
109.286318	2696.167431	5.757888	-0.022400	2.866120
109.283498	2704.218911	5.762893	-0.022405	2.870087
109.755206	2712.286170	5.767898	-0.022499	2.874081
109.964754	2720.306472	5.772902	-0.022544	2.878033
109.922509	2728.360936	5.777907	-0.022543	2.881982
110.227284	2736.389674	5.782912	-0.022605	2.885932
110.375843	2744.409926	5.787917	-0.022639	2.889864
110.846188	2752.462369	5.792922	-0.022733	2.893823
110.770323	2760.518781	5.797926	-0.022724	2.897750
110.944942	2768.567346	5.802931	-0.022763	2.901681
111.243982	2776.610616	5.807936	-0.022825	2.905610
111.284971	2784.638107	5.812941	-0.022838	2.909513
111.514047	2792.771597	5.817946	-0.022887	2.913472
111.749898	2800.765963	5.822950	-0.022937	2.917359
111.889653	2808.775210	5.827955	-0.022969	2.921242
112.137446	2816.782077	5.832960	-0.023021	2.925125
112.344379	2824.797071	5.837965	-0.023066	2.929005
112.637521	2832.863962	5.842970	-0.023126	2.932908
112.650406	2840.911932	5.847974	-0.023135	2.936783
112.879744	2848.929467	5.852979	-0.023184	2.940649
113.243909	2856.921579	5.857984	-0.023257	2.944505
113.333507	2864.979526	5.862989	-0.023280	2.948373
113.611309	2873.057776	5.867994	-0.023338	2.952256
113.804262	2881.088684	5.872998	-0.023380	2.956106
113.769586	2889.106290	5.878003	-0.023379	2.959934
113.908043	2897.164772	5.883008	-0.023411	2.963784
114.241900	2905.155778	5.888013	-0.023479	2.967608
114.494591	2913.237557	5.893018	-0.023532	2.971465
114.674975	2921.270643	5.898022	-0.023572	2.975291
114.844068	2929.292333	5.903027	-0.023610	2.979106
115.108732	2937.340589	5.908032	-0.023665	2.982933
115.202629	2945.367988	5.913037	-0.023688	2.986737
115.601288	2953.396451	5.918042	-0.023769	2.990552
115.806300	2961.473780	5.923046	-0.023813	2.994375
115.934282	2969.493491	5.928051	-0.023843	2.998162
116.102406	2977.526479	5.933056	-0.023880	3.001953
116.264446	2985.538471	5.938061	-0.023916	3.005729
116.506534	2993.573495	5.943066	-0.023967	3.009514
116.446086	3001.671190	5.948070	-0.023962	3.013310
116.629259	3009.682182	5.953075	-0.024002	3.017072
116.859457	3017.712379	5.958080	-0.024051	3.020840
117.003145	3025.705611	5.963085	-0.024084	3.024583
117.193072	3033.766926	5.968090	-0.024125	3.028354
117.503014	3041.809159	5.973094	-0.024189	3.032118
117.618923	3049.864928	5.978099	-0.024217	3.035874
117.617093	3057.891886	5.983104	-0.024222	3.039607
117.823972	3065.903762	5.988109	-0.024267	3.043338
117.960156	3073.949050	5.993114	-0.024298	3.047076
118.202871	3081.991970	5.998118	-0.024349	3.050814
118.290503	3090.020331	6.003123	-0.024372	3.054532
118.754608	3098.044211	6.008128	-0.024464	3.058263
118.867874	3106.069420	6.013133	-0.024491	3.061972
119.074670	3114.127389	6.018138	-0.024536	3.065697
119.358107	3122.133849	6.023142	-0.024595	3.069397
119.616411	3130.251185	6.028147	-0.024649	3.073142
119.755764	3138.304286	6.033152	-0.024681	3.076847
119.964144	3146.258025	6.038157	-0.024726	3.080506
120.266225	3154.274565	6.043162	-0.024788	3.084193
120.303804	3162.314639	6.048166	-0.024801	3.087875
120.422352	3170.391018	6.053171	-0.024829	3.091572
120.696275	3178.421116	6.058176	-0.024886	3.095251
120.885206	3186.403697	6.063181	-0.024927	3.098900
121.036910	3194.449595	6.068186	-0.024961	3.102572
121.139020	3202.518317	6.073190	-0.024987	3.106247
121.427757	3210.529880	6.078195	-0.025046	3.109901
121.655996	3218.577016	6.083200	-0.025095	3.113564
121.624096	3226.605903	6.088205	-0.025095	3.117202
122.023064	3234.617217	6.093210	-0.025175	3.120848
122.259212	3242.605215	6.098214	-0.025225	3.124471
122.360274	3250.666466	6.103219	-0.025250	3.128117
122.579823	3258.744865	6.108224	-0.025297	3.131772
122.531910	3266.771852	6.113229	-0.025294	3.135388
122.844630	3274.791343	6.118234	-0.025358	3.139012
122.986805	3282.812699	6.123238	-0.025391	3.142625
123.311304	3290.842888	6.128243	-0.025457	3.146246
123.584331	3298.874303	6.133248	-0.025514	3.149861
123.603908	3306.948894	6.138253	-0.025524	3.153480
123.926658	3314.969743	6.143258	-0.025590	3.157084
123.783936	3323.010944	6.148262	-0.025569	3.160673
123.814630	3330.996826	6.153267	-0.025581	3.164240
124.199500	3339.042890	6.158272	-0.025659	3.167846
124.393947	3347.066243	6.163277	-0.025701	3.171429
124.685705	3355.109045	6.168282	-0.025761	3.175021
124.770067	3363.143826	6.173286	-0.025783	3.178596
125.110322	3371.163125	6.178291	-0.025852	3.182171
125.420505	3379.188869	6.183296	-0.025916	3.185744
125.526690	3387.212276	6.188301	-0.025942	3.189303
125.925742	3395.281693	6.193306	-0.026022	3.192891
126.228432	3403.303850	6.198310	-0.026085	3.196450
126.089165	3411.334677	6.203315	-0.026065	3.199990
126.389809	3419.353845	6.208320	-0.026127	3.203539
126.422300	3427.365620	6.213325	-0.026139	3.207070
126.492549	3435.446570	6.218330	-0.026158	3.210629
126.537157	3443.480675	6.223334	-0.026172	3.214163
126.868264	3451.478905	6.228339	-0.026240	3.217689
127.134819	3459.540572	6.233344	-0.026296	3.221236
127.131934	3467.524575	6.238349	-0.026301	3.224733
127.487674	3475.562230	6.243354	-0.026373	3.228266
127.643119	3483.658293	6.248358	-0.026408	3.231811
127.749342	3491.712119	6.253363	-0.026434	3.235333
127.883144	3499.697024	6.258368	-0.026465	3.238821
128.199470	3507.674400	6.263373	-0.026530	3.242310
128.558605	3515.729775	6.268378	-0.026603	3.245831
128.469083	3523.743552	6.273382	-0.026592	3.249311
128.590261	3531.806167	6.278387	-0.026621	3.252818
129.048632	3539.836460	6.283392	-0.026712	3.256320
129.145116	3547.843249	6.288397	-0.026736	3.259794
129.457640	3555.843902	6.293402	-0.026800	3.263270
129.532355	3563.891592	6.298406	-0.026820	3.266753
129.438336	3571.940164	6.303411	-0.026809	3.270227
129.885221	3579.988575	6.308416	-0.026898	3.273717
129.869329	3588.002312	6.313421	-0.026901	3.277171
129.974512	3596.020063	6.318426	-0.026927	3.280628
130.210953	3604.010500	6.323430	-0.026977	3.284074
130.357855	3612.062603	6.328435	-0.027010	3.287540
130.601245	3620.114597	6.333440	-0.027061	3.291006
130.411921	3628.154338	6.338445	-0.027032	3.294446
130.686283	3636.167403	6.343450	-0.027089	3.297889
130.897251	3644.197572	6.348454	-0.027135	3.301333
130.837305	3652.200491	6.353459	-0.027129	3.304752
131.036356	3660.252258	6.358464	-0.027173	3.308197
131.449941	3668.271494	6.363469	-0.027256	3.311634
131.589170	3676.344851	6.368474	-0.027288	3.315079
131.818740	3684.333566	6.373478	-0.027336	3.318488
131.897964	3692.357843	6.378483	-0.027357	3.321904
132.345064	3700.348465	6.383488	-0.027446	3.325315
132.421532	3708.370516	6.388493	-0.027467	3.328722
132.339318	3716.474433	6.393498	-0.027457	3.332154
132.875846	3724.476482	6.398502	-0.027563	3.335563
133.039088	3732.474526	6.403507	-0.027600	3.338952
133.251800	3740.530433	6.408512	-0.027645	3.342365
133.284316	3748.534872	6.413517	-0.027657	3.345745
133.520140	3756.581649	6.418522	-0.027707	3.349147
133.512977	3764.661460	6.423526	-0.027712	3.352551
133.674739	3772.693345	6.428531	-0.027748	3.355938
134.334656	3780.670466	6.433536	-0.027877	3.359316
134.347093	3788.681831	6.438541	-0.027885	3.362681
134.415690	3796.748532	6.443546	-0.027904	3.366069
134.652673	3804.748636	6.448550	-0.027954	3.369431
134.618470	3812.814310	6.453555	-0.027954	3.372807
134.757006	3820.891270	6.458560	-0.027986	3.376191
135.012329	3828.827467	6.463565	-0.028039	3.379517
135.350087	3836.830461	6.468570	-0.028108	3.382870
135.359753	3844.907505	6.473574	-0.028116	3.386240
135.498147	3852.927771	6.478579	-0.028148	3.389586
135.762400	3861.029489	6.483584	-0.028203	3.392968
135.959473	3869.054928	6.488589	-0.028246	3.396312
135.898458	3877.052860	6.493594	-0.028240	3.399633
136.194677	3885.011419	6.498598	-0.028302	3.402946
136.287430	3893.036286	6.503603	-0.028325	3.406277
136.489953	3901.072747	6.508608	-0.028369	3.409613
136.684692	3909.102731	6.513613	-0.028411	3.412942
137.031336	3917.134123	6.518618	-0.028481	3.416275
137.132251	3925.143912	6.523622	-0.028506	3.419586
137.275542	3933.145916	6.528627	-0.028539	3.422893
137.584768	3941.194376	6.533632	-0.028603	3.426221
137.732577	3949.215512	6.538637	-0.028636	3.429529
137.824409	3957.297646	6.543642	-0.028659	3.432857
137.833157	3965.345058	6.548646	-0.028667	3.436165
137.928349	3973.313318	6.553651	-0.028691	3.439439
137.986354	3981.374486	6.558656	-0.028707	3.442748
138.153111	3989.363744	6.563661	-0.028745	3.446028
138.512435	3997.380222	6.568666	-0.028817	3.449322
138.581015	4005.447851	6.573670	-0.028836	3.452624
138.677976	4013.501851	6.578675	-0.028860	3.455918
138.919100	4021.501516	6.583680	-0.028911	3.459192
138.939916	4029.536482	6.588685	-0.028921	3.462470
139.188132	4037.560912	6.593690	-0.028973	3.465748
139.348150	4045.589350	6.598694	-0.029009	3.469021
139.619734	4053.606600	6.603699	-0.029066	3.472290
139.794081	4061.687686	6.608704	-0.029104	3.475579
139.809670	4069.648258	6.613709	-0.029113	3.478811
139.986039	4077.694446	6.618714	-0.029152	3.482080
139.976287	4085.698178	6.623718	-0.029156	3.485323
140.157283	4093.705963	6.628723	-0.029196	3.488570
140.482585	4101.764836	6.633728	-0.029263	3.491839
140.702367	4109.761583	6.638733	-0.029309	3.495077
140.889309	4117.788535	6.643738	-0.029350	3.498323
140.983989	4125.839507	6.648742	-0.029374	3.501573
141.163861	4133.805346	6.653747	-0.029413	3.504788
141.402911	4141.881100	6.658752	-0.029464	3.508046
141.503132	4149.894417	6.663757	-0.029489	3.511271
141.973676	4157.897535	6.668762	-0.029582	3.514501
142.214801	4165.930525	6.673766	-0.029633	3.517733
142.233012	4173.957719	6.678771	-0.029643	3.520953
142.562860	4181.934168	6.683776	-0.029710	3.524159
142.847840	4189.982324	6.688781	-0.029769	3.527389
143.033531	4198.044764	6.693786	-0.029810	3.530619
143.136138	4206.072510	6.698790	-0.029835	3.533830
143.297196	4214.125886	6.703795	-0.029871	3.537050
143.455075	4222.151679	6.708800	-0.029906	3.540256
143.427060	4230.144723	6.713805	-0.029907	3.543440
143.639822	4238.182593	6.718810	-0.029953	3.546646
143.666403	4246.232353	6.723814	-0.029964	3.549848
143.821766	4254.348175	6.728819	-0.029999	3.553078
144.218884	4262.367710	6.733824	-0.030079	3.556274
144.390894	4270.293246	6.738829	-0.030117	3.559423
144.417619	4278.313095	6.743834	-0.030128	3.562602
144.515578	4286.347490	6.748838	-0.030152	3.565786
144.861670	4294.327414	6.753843	-0.030222	3.568953
145.047778	4302.405374	6.758848	-0.030263	3.572151
144.999094	4310.427983	6.763853	-0.030260	3.575318
145.523240	4318.423745	6.768858	-0.030364	3.578488
145.600349	4326.457049	6.773862	-0.030384	3.581656
145.601157	4334.445162	6.778867	-0.030390	3.584802
145.822332	4342.489416	6.783872	-0.030437	3.587974
145.996435	4350.524438	6.788877	-0.030476	3.591138
146.007657	4358.564861	6.793882	-0.030484	3.594296
146.031615	4366.589170	6.798886	-0.030494	3.597446
146.187940	4374.557665	6.803891	-0.030529	3.600575
146.731921	4382.585969	6.808896	-0.030637	3.603736
146.756132	4390.598005	6.813901	-0.030647	3.606872
146.765167	4398.653257	6.818906	-0.030655	3.610023
147.081372	4406.687372	6.823910	-0.030720	3.613171
147.183267	4414.705402	6.828915	-0.030745	3.616303
147.207762	4422.733499	6.833920	-0.030755	3.619435
147.490116	4430.731191	6.838925	-0.030814	3.622560
147.706562	4438.771833	6.843930	-0.030860	3.625697
147.621216	4446.842267	6.848934	-0.030851	3.628834
147.845827	4454.836956	6.853939	-0.030898	3.631947
148.159507	4462.892739	6.858944	-0.030963	3.635084
147.994208	4470.894683	6.863949	-0.030938	3.638185
148.247864	4478.940463	6.868954	-0.030991	3.641311
148.516860	4486.903523	6.873958	-0.031047	3.644403
148.363476	4494.955800	6.878963	-0.031025	3.647515
148.627008	4503.001637	6.883968	-0.031080	3.650633
148.830836	4511.013294	6.888973	-0.031124	3.653734
149.035665	4519.060916	6.893978	-0.031168	3.656846
149.031070	4527.084391	6.898982	-0.031173	3.659941
149.225347	4535.089017	6.903987	-0.031215	3.663030
149.462177	4543.155213	6.908992	-0.031266	3.666142
149.644174	4551.079443	6.913997	-0.031305	3.669196
149.939061	4559.186410	6.919002	-0.031366	3.672320
150.016593	4567.196259	6.924006	-0.031387	3.675398
150.208198	4575.171055	6.929011	-0.031428	3.678463
150.316238	4583.225780	6.934016	-0.031455	3.681554
150.231661	4591.203929	6.939021	-0.031445	3.684608
150.418767	4599.270214	6.944026	-0.031486	3.687701
150.404265	4607.306050	6.949030	-0.031489	3.690774
150.782786	4615.316970	6.954035	-0.031566	3.693845
151.066738	4623.340946	6.959040	-0.031624	3.696915
150.975841	4631.302126	6.964045	-0.031613	3.699950
151.197690	4639.363284	6.969050	-0.031661	3.703029
151.384805	4647.367093	6.974054	-0.031702	3.706082
151.324233	4655.399416	6.979059	-0.031696	3.709137
151.311385	4663.509186	6.984064	-0.031700	3.712220
151.477686	4671.591122	6.989069	-0.031737	3.715295
151.869090	4679.525479	6.994074	-0.031816	3.718316
151.854615	4687.538616	6.999078	-0.031819	3.721355
151.987016	4695.474740	7.004083	-0.031850	3.724366
152.425059	4703.557061	7.009088	-0.031937	3.727437
152.510955	4711.527467	7.014093	-0.031959	3.730455
152.491349	4719.599460	7.019098	-0.031962	3.733506
152.523767	4727.650792	7.024102	-0.031974	3.736548
152.651912	4735.619927	7.029107	-0.032004	3.739559
153.031184	4743.655980	7.034112	-0.032080	3.742598
153.046586	4751.658518	7.039117	-0.032089	3.745614
153.371021	4759.717925	7.044122	-0.032156	3.748656
153.246888	4767.773736	7.049126	-0.032139	3.751684
153.522058	4775.720686	7.054131	-0.032196	3.754678
154.020898	4783.771715	7.059136	-0.032295	3.757713
154.002679	4791.773119	7.064141	-0.032297	3.760716
154.058996	4799.833811	7.069146	-0.032314	3.763740
154.418284	4807.845795	7.074150	-0.032387	3.766750
154.544247	4815.836045	7.079155	-0.032416	3.769744
154.672786	4823.921058	7.084160	-0.032446	3.772772
154.773090	4831.951672	7.089165	-0.032471	3.775776
155.197713	4839.949900	7.094170	-0.032556	3.778772
155.335398	4847.977816	7.099174	-0.032588	3.781771
155.370842	4855.965543	7.104179	-0.032600	3.784751
155.618473	4864.063409	7.109184	-0.032652	3.787774
155.663017	4872.040711	7.114189	-0.032667	3.790744
155.883156	4880.100338	7.119194	-0.032714	3.793747
155.995815	4888.141736	7.124198	-0.032741	3.796739
156.188430	4896.048580	7.129203	-0.032783	3.799680
156.139932	4904.100393	7.134208	-0.032780	3.802667
156.366161	4912.081761	7.139213	-0.032828	3.805632
156.665018	4920.125058	7.144218	-0.032889	3.808619
156.770201	4928.172602	7.149222	-0.032915	3.811600
156.767649	4936.215033	7.154227	-0.032921	3.814576
157.160651	4944.212963	7.159232	-0.033000	3.817541
157.293355	4952.219630	7.164237	-0.033030	3.820501
157.252703	4960.252699	7.169242	-0.033029	3.823465
157.450726	4968.261373	7.174246	-0.033072	3.826423
157.606168	4976.260973	7.179251	-0.033107	3.829374
157.810626	4984.336127	7.184256	-0.033151	3.832352
157.698257	4992.335470	7.189261	-0.033136	3.835293
158.094230	5000.318965	7.194266	-0.033216	3.838236
158.278557	5008.381907	7.199270	-0.033256	3.841202
158.405794	5016.341215	7.204275	-0.033286	3.844126
158.503671	5024.418133	7.209280	-0.033310	3.847091
158.577436	5032.403828	7.214285	-0.033330	3.850019
158.639319	5040.461116	7.219290	-0.033347	3.852972
158.798691	5048.524342	7.224294	-0.033383	3.855926
158.925082	5056.500844	7.229299	-0.033412	3.858845
159.274861	5064.538690	7.234304	-0.033484	3.861789
159.189454	5072.540810	7.239309	-0.033474	3.864709
159.341465	5080.622453	7.244314	-0.033508	3.867661
159.447411	5088.628035	7.249318	-0.033534	3.870581
159.676127	5096.804538	7.254323	-0.033583	3.873564
159.855540	5104.868275	7.259328	-0.033622	3.876503
160.035783	5112.732087	7.264333	-0.033661	3.879367
160.090760	5120.745144	7.269338	-0.033678	3.882280
160.055417	5128.717482	7.274342	-0.033677	3.885175
160.358351	5136.756065	7.279347	-0.033740	3.888098
160.471393	5144.796268	7.284352	-0.033767	3.891016
160.392937	5152.795798	7.289357	-0.033758	3.893913
160.835544	5160.786762	7.294362	-0.033846	3.896815
161.112804	5168.783924	7.299366	-0.033904	3.899714
161.205001	5176.799427	7.304371	-0.033927	3.902614
161.381173	5184.849419	7.309376	-0.033966	3.905525
161.594224	5192.868119	7.314381	-0.034012	3.908424
161.811991	5200.894360	7.319386	-0.034058	3.911323
162.009500	5208.945030	7.324390	-0.034101	3.914229
162.069541	5216.907377	7.329395	-0.034118	3.917098
162.370297	5224.943128	7.334400	-0.034180	3.919996
162.266560	5232.949976	7.339405	-0.034167	3.922874
162.637937	5240.969860	7.344410	-0.034242	3.925763
162.922713	5248.982801	7.349414	-0.034301	3.928646
163.004085	5257.025919	7.354419	-0.034322	3.931534
163.185082	5265.067387	7.359424	-0.034362	3.934421
163.444601	5273.062119	7.364429	-0.034416	3.937290
163.384142	5281.050804	7.369434	-0.034411	3.940149
163.450523	5289.099220	7.374438	-0.034430	3.943030
163.731062	5297.129015	7.379443	-0.034488	3.945906
164.076957	5305.142354	7.384448	-0.034558	3.948776
164.135146	5313.169638	7.389453	-0.034575	3.951642
164.143230	5321.238495	7.394458	-0.034583	3.954521
164.512226	5329.238772	7.399462	-0.034657	3.957380
164.527321	5337.213021	7.404467	-0.034666	3.960221
164.660688	5345.183804	7.409472	-0.034697	3.963061
165.014385	5353.217402	7.414477	-0.034769	3.965924
164.914364	5361.262833	7.419482	-0.034756	3.968783
165.100054	5369.314501	7.424486	-0.034797	3.971646
165.321482	5377.305260	7.429491	-0.034844	3.974486
165.557849	5385.350443	7.434496	-0.034894	3.977343
165.680309	5393.334619	7.439501	-0.034923	3.980175
165.805155	5401.374693	7.444506	-0.034952	3.983025
166.061190	5409.403000	7.449510	-0.035006	3.985871
166.069104	5417.408060	7.454515	-0.035013	3.988702
166.273468	5425.476015	7.459520	-0.035057	3.991557
166.399008	5433.489798	7.464525	-0.035087	3.994389
166.663634	5441.533929	7.469530	-0.035142	3.997232
166.595668	5449.522929	7.474534	-0.035135	4.000049
166.855784	5457.507944	7.479539	-0.035190	4.002867
167.158590	5465.526926	7.484544	-0.035252	4.005696
167.212062	5473.592237	7.489549	-0.035268	4.008535
167.335486	5481.622857	7.494554	-0.035297	4.011361
167.471017	5489.648885	7.499558	-0.035329	4.014184
167.676499	5497.681964	7.504563	-0.035373	4.017008
167.882217	5505.666490	7.509568	-0.035417	4.019813
168.122129	5513.679229	7.514573	-0.035468	4.022626
168.329788	5521.670583	7.519578	-0.035512	4.025430
168.421715	5529.718147	7.524582	-0.035536	4.028250
168.315738	5537.736275	7.529587	-0.035522	4.031054
168.453900	5545.897637	7.534592	-0.035554	4.033910
168.621235	5553.871432	7.539597	-0.035591	4.036699
168.926329	5561.760836	7.544602	-0.035654	4.039458
169.021209	5569.814217	7.549606	-0.035677	4.042270
169.101937	5577.794146	7.554611	-0.035698	4.045054
169.301958	5585.841782	7.559616	-0.035742	4.047861
169.353126	5593.843074	7.564621	-0.035757	4.050648
169.592353	5601.864456	7.569626	-0.035808	4.053443
169.717510	5609.924088	7.574630	-0.035837	4.056247
169.822505	5617.883247	7.579635	-0.035863	4.059015
170.218168	5625.932997	7.584640	-0.035942	4.061816
170.362021	5633.924146	7.589645	-0.035975	4.064591
170.413216	5641.966051	7.594650	-0.035991	4.067380
170.634003	5649.990369	7.599654	-0.036038	4.070164
170.763186	5658.018588	7.604659	-0.036068	4.072946
170.901895	5666.057390	7.609664	-0.036100	4.075730
170.825084	5674.017400	7.614669	-0.036091	4.078482
171.249417	5682.045856	7.619674	-0.036176	4.081262
171.368484	5690.045100	7.624678	-0.036205	4.084027
171.398791	5698.089536	7.629683	-0.036216	4.086803
171.674559	5706.116205	7.634688	-0.036274	4.089575
171.609362	5714.133727	7.639693	-0.036267	4.092338
171.755902	5722.165613	7.644698	-0.036301	4.095106
171.896841	5730.195962	7.649702	-0.036333	4.097872
172.125171	5738.168498	7.654707	-0.036382	4.100617
172.445708	5746.233798	7.659712	-0.036447	4.103393
172.410821	5754.259198	7.664717	-0.036447	4.106149
172.616739	5762.242605	7.669722	-0.036491	4.108892
172.668826	5770.329224	7.674726	-0.036507	4.111667
172.826461	5778.349939	7.679731	-0.036542	4.114418
173.176745	5786.411730	7.684736	-0.036613	4.117184
173.117204	5794.340190	7.689741	-0.036608	4.119898
173.376927	5802.340533	7.694746	-0.036663	4.122638
173.571445	5810.369733	7.699750	-0.036705	4.125385
173.622966	5818.378540	7.704755	-0.036721	4.128122
173.820744	5826.487065	7.709760	-0.036763	4.130893
173.855021	5834.489891	7.714765	-0.036776	4.133624
174.190539	5842.474330	7.719770	-0.036844	4.136350
174.430191	5850.460295	7.724774	-0.036895	4.139074
174.489992	5858.528679	7.729779	-0.036912	4.141822
174.618131	5866.510998	7.734784	-0.036942	4.144540
174.976549	5874.524464	7.739789	-0.037015	4.147269
175.176248	5882.540671	7.744794	-0.037058	4.149995
175.409485	5890.615330	7.749798	-0.037107	4.152740
175.407563	5898.601457	7.754803	-0.037113	4.155451
175.395323	5906.630919	7.759808	-0.037117	4.158174
175.415298	5914.640583	7.764813	-0.037126	4.160888
175.770180	5922.616391	7.769818	-0.037199	4.163594
175.951969	5930.644943	7.774822	-0.037238	4.166314
176.178165	5938.650549	7.779827	-0.037287	4.169024
176.444471	5946.746044	7.784832	-0.037342	4.171764
176.566110	5954.706660	7.789837	-0.037371	4.174454
176.562872	5962.769127	7.794842	-0.037376	4.177176
176.581733	5970.767628	7.799846	-0.037386	4.179875
176.847599	5978.749317	7.804851	-0.037441	4.182569
177.012419	5986.783131	7.809856	-0.037478	4.185277
177.080333	5994.793832	7.814861	-0.037497	4.187975
177.408349	6002.780936	7.819866	-0.037564	4.190666
177.633782	6010.952134	7.824870	-0.037612	4.193417
177.593376	6018.915146	7.829875	-0.037610	4.196092
177.725235	6026.889873	7.834880	-0.037641	4.198772
177.811374	6034.948429	7.839885	-0.037663	4.201477
177.994524	6042.849969	7.844890	-0.037703	4.204129
178.338272	6050.945394	7.849894	-0.037773	4.206847
178.396760	6058.879726	7.854899	-0.037790	4.209505
178.584604	6066.982134	7.859904	-0.037831	4.212219
178.517599	6074.999598	7.864909	-0.037824	4.214901
178.801993	6083.009643	7.869914	-0.037883	4.217582
178.888959	6091.026175	7.874918	-0.037906	4.220261
178.832955	6098.984775	7.879923	-0.037901	4.222918
179.118574	6107.018719	7.884928	-0.037960	4.225601
179.208346	6115.034641	7.889933	-0.037983	4.228275
179.388696	6123.069897	7.894938	-0.038023	4.230955
179.469802	6131.151665	7.899942	-0.038044	4.233647
179.762918	6139.117078	7.904947	-0.038104	4.236301
180.125004	6147.138214	7.909952	-0.038178	4.238973
180.045359	6155.136765	7.914957	-0.038169	4.241631
180.052744	6163.113403	7.919962	-0.038176	4.244281
180.496898	6171.159887	7.924966	-0.038265	4.246956
180.356972	6179.150768	7.929971	-0.038245	4.249606
180.336768	6187.232745	7.934976	-0.038247	4.252286
180.714568	6195.224977	7.939981	-0.038324	4.254938
180.987206	6203.240324	7.944986	-0.038380	4.257595
181.138531	6211.312218	7.949990	-0.038415	4.260267
181.164471	6219.294431	7.954995	-0.038425	4.262908
181.326662	6227.323317	7.960000	-0.038462	4.265563
181.333983	6235.333033	7.965005	-0.038469	4.268209
181.665480	6243.373237	7.970010	-0.038537	4.270866
181.969963	6251.422140	7.975014	-0.038600	4.273524
181.918826	6259.464590	7.980019	-0.038596	4.276175
182.041671	6267.425073	7.985024	-0.038625	4.278799
182.153238	6275.471404	7.990029	-0.038652	4.281450
182.316208	6283.419928	7.995034	-0.038688	4.284067
182.374834	6291.479521	8.000038	-0.038705	4.286718
182.634927	6299.456433	8.005043	-0.038759	4.289342
182.886189	6307.553603	8.010048	-0.038812	4.292004
182.867933	6315.565512	8.015053	-0.038815	4.294634
182.863409	6323.568671	8.020058	-0.038820	4.297260
183.082339	6331.577032	8.025062	-0.038867	4.299887
183.176408	6339.547642	8.030067	-0.038890	4.302500
183.344116	6347.579562	8.035072	-0.038928	4.305131
183.367310	6355.597943	8.040077	-0.038938	4.307756
183.558439	6363.637345	8.045082	-0.038979	4.310386
183.545690	6371.707507	8.050086	-0.038983	4.313024
183.640215	6379.697922	8.055091	-0.039007	4.315635
184.018645	6387.704904	8.060096	-0.039083	4.318252
184.063293	6395.723518	8.065101	-0.039098	4.320869
184.178264	6403.650620	8.070106	-0.039125	4.323454
184.368159	6411.736103	8.075110	-0.039166	4.326090
184.523063	6419.720936	8.080115	-0.039201	4.328692
184.570951	6427.802223	8.085120	-0.039216	4.331323
184.743103	6435.807025	8.090125	-0.039254	4.333928
185.000465	6443.845631	8.095130	-0.039308	4.336543
185.105908	6451.800160	8.100134	-0.039334	4.339128
185.143189	6459.820557	8.105139	-0.039347	4.341732
185.339147	6467.820337	8.110144	-0.039389	4.344329
185.246327	6475.870463	8.115149	-0.039378	4.346939
185.538365	6483.859679	8.120154	-0.039438	4.349530
185.740330	6491.939501	8.125158	-0.039482	4.352149
185.804764	6499.956624	8.130163	-0.039500	4.354745
185.944654	6508.002158	8.135168	-0.039532	4.357348
186.184021	6515.950150	8.140173	-0.039583	4.359920
186.405780	6523.928411	8.145178	-0.039630	4.362499
186.696636	6531.933363	8.150182	-0.039690	4.365086
186.867298	6539.952268	8.155187	-0.039728	4.367675
187.009184	6547.989141	8.160192	-0.039760	4.370268
187.060355	6556.022871	8.165197	-0.039776	4.372858
187.186099	6564.053222	8.170202	-0.039805	4.375446
187.447117	6572.080077	8.175206	-0.039860	4.378032
187.462991	6580.041524	8.180211	-0.039869	4.380594
187.499734	6588.073306	8.185216	-0.039882	4.383177
187.858701	6596.072044	8.190221	-0.039954	4.385750
187.968458	6604.126691	8.195226	-0.039981	4.388338
188.151305	6612.159579	8.200230	-0.040021	4.390917
187.949926	6620.163011	8.205235	-0.039990	4.393484
188.037322	6628.199247	8.210240	-0.040012	4.396061
188.191481	6636.165053	8.215245	-0.040047	4.398615
188.409842	6644.231026	8.220250	-0.040093	4.401199
188.742545	6652.188726	8.225254	-0.040161	4.403748
188.671394	6660.223154	8.230259	-0.040154	4.406318
188.785691	6668.268066	8.235264	-0.040181	4.408890
188.941710	6676.301430	8.240269	-0.040216	4.411458
189.227659	6684.315994	8.245274	-0.040276	4.414018
189.472053	6692.377078	8.250278	-0.040327	4.416592
189.509968	6700.306111	8.255283	-0.040340	4.419121
189.714585	6708.429216	8.260288	-0.040384	4.421712
190.030832	6716.328087	8.265293	-0.040449	4.424229
189.921926	6724.400664	8.270298	-0.040435	4.426799
190.114366	6732.454878	8.275302	-0.040477	4.429363
190.237930	6740.456893	8.280307	-0.040506	4.431908
190.323880	6748.471959	8.285312	-0.040528	4.434456
190.414250	6756.519143	8.290317	-0.040551	4.437013
190.481825	6764.476892	8.295322	-0.040569	4.439539
190.582271	6772.542113	8.300326	-0.040594	4.442099
190.565246	6780.434363	8.305331	-0.040597	4.444601
190.884356	6788.563137	8.310336	-0.040662	4.447179
191.097420	6796.510804	8.315341	-0.040708	4.449697
191.265007	6804.599788	8.320346	-0.040745	4.452258
191.459562	6812.588534	8.325350	-0.040787	4.454787
191.686777	6820.624958	8.330355	-0.040836	4.457329
191.955031	6828.628017	8.335360	-0.040892	4.459859
191.974011	6836.667396	8.340365	-0.040901	4.462398
192.102252	6844.613126	8.345370	-0.040931	4.464906
192.368070	6852.728099	8.350374	-0.040987	4.467467
192.351022	6860.671784	8.355379	-0.040989	4.469972
192.423336	6868.713077	8.360384	-0.041009	4.472506
192.513651	6876.731005	8.365389	-0.041032	4.475031
192.383932	6884.732073	8.370394	-0.041014	4.477549
192.721276	6892.718746	8.375398	-0.041082	4.480063
192.877095	6900.756638	8.380403	-0.041117	4.482590
192.962298	6908.753147	8.385408	-0.041139	4.485103
193.188535	6916.784591	8.390413	-0.041187	4.487626
193.483413	6924.763263	8.395418	-0.041248	4.490131
193.451119	6932.856196	8.400422	-0.041248	4.492670
193.319237	6940.839094	8.405427	-0.041230	4.495172
193.655510	6948.884856	8.410432	-0.041298	4.497694
193.861699	6956.850691	8.415437	-0.041343	4.500189
193.922442	6964.859245	8.420442	-0.041360	4.502696
194.039198	6972.897767	8.425446	-0.041388	4.505210
194.231707	6980.887251	8.430451	-0.041430	4.507709
194.557122	6988.951115	8.435456	-0.041496	4.510229
194.445976	6997.020157	8.440461	-0.041482	4.512748
194.533045	7005.015063	8.445466	-0.041504	4.515244
194.557349	7013.022928	8.450470	-0.041514	4.517742
194.752047	7020.970857	8.455475	-0.041557	4.520220
194.832930	7029.041331	8.460480	-0.041578	4.522735
195.145287	7036.966272	8.465485	-0.041642	4.525203
195.117058	7045.035493	8.470490	-0.041643	4.527715
195.320106	7053.060452	8.475494	-0.041687	4.530211
195.326556	7061.057057	8.480499	-0.041694	4.532697
195.629657	7069.096387	8.485504	-0.041756	4.535196
195.698678	7077.090430	8.490509	-0.041775	4.537679
195.970575	7085.107804	8.495514	-0.041832	4.540167
196.304729	7093.115242	8.500518	-0.041900	4.542652
196.035880	7101.106379	8.505523	-0.041856	4.545129
196.130157	7109.167357	8.510528	-0.041879	4.547627
196.351301	7117.149470	8.515533	-0.041927	4.550099
196.568653	7125.226845	8.520538	-0.041973	4.552600
196.512069	7133.268674	8.525542	-0.041969	4.555087
196.556119	7141.233621	8.530547	-0.041983	4.557550
196.997561	7149.224401	8.535552	-0.042071	4.560020
197.063684	7157.267784	8.540557	-0.042089	4.562504
197.141430	7165.216390	8.545562	-0.042110	4.564957
197.205942	7173.316142	8.550566	-0.042128	4.567456
197.352322	7181.259030	8.555571	-0.042161	4.569905
197.587925	7189.353893	8.560576	-0.042211	4.572400
197.743148	7197.360256	8.565581	-0.042246	4.574866
197.821407	7205.357039	8.570586	-0.042266	4.577328
198.011914	7213.372060	8.575591	-0.042308	4.579794
198.124700	7221.444499	8.580595	-0.042335	4.582276
198.461656	7229.407015	8.585600	-0.042404	4.584724
198.357461	7237.466419	8.590605	-0.042390	4.587199
198.563601	7245.401337	8.595610	-0.042435	4.589635
198.683688	7253.498476	8.600615	-0.042463	4.592120
198.804595	7261.518588	8.605619	-0.042492	4.594579
198.960601	7269.615345	8.610624	-0.042527	4.597061
199.071680	7277.516793	8.615629	-0.042553	4.599481
199.123270	7285.535738	8.620634	-0.042569	4.601937
199.228642	7293.495674	8.625639	-0.042595	4.604372
199.358799	7301.552776	8.630643	-0.042625	4.606837
199.696247	7309.562046	8.635648	-0.042694	4.609285
199.804003	7317.604406	8.640653	-0.042720	4.611742
200.020637	7325.639845	8.645658	-0.042766	4.614195
200.142214	7333.692949	8.650663	-0.042795	4.616653
200.137032	7341.599863	8.655667	-0.042800	4.619065
200.208813	7349.658462	8.660672	-0.042819	4.621522
200.439699	7357.641549	8.665677	-0.042868	4.623954
200.719790	7365.705891	8.670682	-0.042926	4.626410
200.795691	7373.702599	8.675687	-0.042947	4.628844
200.705186	7381.757753	8.680691	-0.042936	4.631294
200.882012	7389.796994	8.685696	-0.042975	4.633738
201.091054	7397.763537	8.690701	-0.043020	4.636159
201.224056	7405.718772	8.695706	-0.043050	4.638575
201.353062	7413.797539	8.700711	-0.043080	4.641028
201.376782	7421.740424	8.705715	-0.043091	4.643437
201.379118	7429.782144	8.710720	-0.043097	4.645876
201.461086	7437.804609	8.715725	-0.043119	4.648307
201.900848	7445.833353	8.720730	-0.043206	4.650739
202.050688	7453.865608	8.725735	-0.043240	4.653171
201.958531	7461.853886	8.730739	-0.043229	4.655588
202.158460	7469.916460	8.735744	-0.043272	4.658027
202.382049	7477.911117	8.740749	-0.043320	4.660443
202.522967	7485.902470	8.745754	-0.043352	4.662857
202.708907	7493.912686	8.750759	-0.043393	4.665276
202.706011	7501.922214	8.755763	-0.043398	4.667693
202.969257	7509.971227	8.760768	-0.043453	4.670121
203.097024	7518.037387	8.765773	-0.043483	4.672553
203.170251	7526.072313	8.770778	-0.043503	4.674974
203.350627	7534.077757	8.775783	-0.043543	4.677384
203.475730	7542.021770	8.780787	-0.043572	4.679776
203.659832	7550.048063	8.785792	-0.043612	4.682190
203.556867	7557.987682	8.790797	-0.043599	4.684578
203.708233	7566.085512	8.795802	-0.043633	4.687012
203.765916	7574.085189	8.800807	-0.043650	4.689415
204.085325	7582.076041	8.805811	-0.043715	4.691813
204.183883	7590.134239	8.810816	-0.043740	4.694231
204.326128	7598.165688	8.815821	-0.043772	4.696640
204.625357	7606.083624	8.820826	-0.043834	4.699013
204.881355	7614.182569	8.825831	-0.043888	4.701439
204.871583	7622.135845	8.830835	-0.043892	4.703821
205.209123	7630.193761	8.835840	-0.043961	4.706232
205.086231	7638.205529	8.840845	-0.043944	4.708629
205.101892	7646.227628	8.845850	-0.043953	4.711028
205.380206	7654.238135	8.850855	-0.044011	4.713421
205.472233	7662.253419	8.855859	-0.044034	4.715815
205.727439	7670.286720	8.860864	-0.044087	4.718212
205.566853	7678.229651	8.865869	-0.044063	4.720583
205.589220	7686.229411	8.870874	-0.044074	4.722969
206.016440	7694.323765	8.875879	-0.044159	4.725381
206.154700	7702.296137	8.880883	-0.044191	4.727756
206.238840	7710.364363	8.885888	-0.044213	4.730158
206.165757	7718.381740	8.890893	-0.044205	4.732544
206.369176	7726.420504	8.895898	-0.044249	4.734935
206.541402	7734.471514	8.900903	-0.044287	4.737329
206.626192	7742.391293	8.905907	-0.044309	4.739682
206.690728	7750.431541	8.910912	-0.044327	4.742070
206.767001	7758.404471	8.915917	-0.044347	4.744437
206.996309	7766.449344	8.920922	-0.044396	4.746823
207.313566	7774.523529	8.925927	-0.044461	4.749217
207.095491	7782.491745	8.930931	-0.044426	4.751580
207.240720	7790.583853	8.935936	-0.044459	4.753977
207.499738	7798.575955	8.940941	-0.044513	4.756342
207.721256	7806.480976	8.945946	-0.044561	4.758681
207.816597	7814.529941	8.950951	-0.044584	4.761062
207.860280	7822.532727	8.955955	-0.044599	4.763428
208.099885	7830.547184	8.960960	-0.044649	4.765796
208.263303	7838.584872	8.965965	-0.044686	4.768170
208.244301	7846.577810	8.970970	-0.044688	4.770530
208.449073	7854.693965	8.975975	-0.044732	4.772924
208.505631	7862.626024	8.980979	-0.044749	4.775263
208.728619	7870.649991	8.985984	-0.044796	4.777628
208.860298	7878.631239	8.990989	-0.044827	4.779979
209.177813	7886.714419	8.995994	-0.044892	4.782358
209.300037	7894.724817	9.000999	-0.044921	4.784716
209.324719	7902.699654	9.006003	-0.044931	4.787062
209.453835	7910.702196	9.011008	-0.044961	4.789415
209.525140	7918.747216	9.016013	-0.044981	4.791779
209.716195	7926.762903	9.021018	-0.045022	4.794133
209.796832	7934.813959	9.026023	-0.045043	4.796497
209.707150	7942.761154	9.031027	-0.045033	4.798829
209.760045	7950.796311	9.036032	-0.045049	4.801186
210.141616	7958.796796	9.041037	-0.045126	4.803530
210.173245	7966.800194	9.046042	-0.045137	4.805876
210.435872	7974.838861	9.051047	-0.045192	4.808229
210.485182	7982.790727	9.056051	-0.045208	4.810557
210.821480	7990.290065	9.061056	-0.045276	4.812750
210.901480	7994.825298	9.066061	-0.045294	4.814076

210.787219	7997.332203	9.071066	-0.045276	4.814809
211.154108	7998.726177	9.076071	-0.045346	4.815215
211.191619	7999.158214	9.081075	-0.045354	4.815341
211.280635	8000.151687	9.086080	-0.045372	4.815631
211.314405	8000.148035	9.091085	-0.045379	4.815630
211.245546	8000.042339	9.096090	-0.045367	4.815600
211.281510	8000.108128	9.101095	-0.045374	4.815619
211.333396	8000.070601	9.106099	-0.045385	4.815607
211.563201	8000.084021	9.111104	-0.045428	4.815610
211.439767	8000.129064	9.116109	-0.045406	4.815624
211.374973	8000.104586	9.121114	-0.045395	4.815617
211.637558	8000.123879	9.126119	-0.045444	4.815621
211.818393	8000.108739	9.131123	-0.045479	4.815616
211.959476	8000.126055	9.136128	-0.045506	4.815621
211.879626	8000.114145	9.141133	-0.045492	4.815617
211.989446	8000.089307	9.146138	-0.045513	4.815610
211.942080	8000.167623	9.151143	-0.045505	4.815633
211.939747	8000.209299	9.156147	-0.045505	4.815645
212.071886	8000.139976	9.161152	-0.045531	4.815624
211.929198	8000.162281	9.166157	-0.045505	4.815631
211.883224	8000.119956	9.171162	-0.045497	4.815619
212.277264	8000.171290	9.176167	-0.045571	4.815632
212.061520	8000.145422	9.181171	-0.045532	4.815626
212.004881	8000.103991	9.186176	-0.045522	4.815614
212.067973	8000.121104	9.191181	-0.045535	4.815618
211.928259	8000.034541	9.196186	-0.045510	4.815594
212.169340	8000.097265	9.201191	-0.045555	4.815611
212.162321	8000.085474	9.206195	-0.045555	4.815607
212.482509	8000.114249	9.211200	-0.045615	4.815614
212.437156	8000.111444	9.216205	-0.045607	4.815614
212.483018	8000.133616	9.221210	-0.045617	4.815620
212.526054	8000.192049	9.226215	-0.045626	4.815637
212.324037	8000.129029	9.231219	-0.045589	4.815619
212.520553	8000.162198	9.236224	-0.045626	4.815628
212.460217	8000.136724	9.241229	-0.045616	4.815621
212.496613	8000.123504	9.246234	-0.045623	4.815617
212.436509	8000.203749	9.251239	-0.045613	4.815641
212.298248	8000.106529	9.256243	-0.045588	4.815613
212.570641	8000.130255	9.261248	-0.045639	4.815618
212.495825	8000.177158	9.266253	-0.045626	4.815632
212.450102	8000.138040	9.271258	-0.045619	4.815621
212.503479	8000.191303	9.276263	-0.045629	4.815636
212.467662	8000.136329	9.281267	-0.045623	4.815621
212.574861	8000.126397	9.286272	-0.045644	4.815617
212.587887	8000.158714	9.291277	-0.045647	4.815626
212.863446	8000.153661	9.296282	-0.045700	4.815624
212.880391	8000.263994	9.301287	-0.045704	4.815656
212.899037	8000.217381	9.306291	-0.045708	4.815642
213.182882	8000.187904	9.311296	-0.045761	4.815632
212.922095	8000.194402	9.316301	-0.045714	4.815635
212.837713	8000.227267	9.321306	-0.045699	4.815645
213.051452	8000.220140	9.326311	-0.045739	4.815642
213.000864	8000.163857	9.331315	-0.045731	4.815626
212.841402	8000.143174	9.336320	-0.045702	4.815621
212.779512	8000.187085	9.341325	-0.045691	4.815634
212.804585	8000.198240	9.346330	-0.045696	4.815637
212.890329	8000.217860	9.351335	-0.045713	4.815642
212.741252	8000.126869	9.356339	-0.045686	4.815616
212.957677	8000.093089	9.361344	-0.045727	4.815605
212.873980	8000.117422	9.366349	-0.045712	4.815613
212.743313	8000.126041	9.371354	-0.045689	4.815616
212.775275	8000.159734	9.376359	-0.045696	4.815626
212.863953	8000.104652	9.381363	-0.045713	4.815609
213.113593	8000.117330	9.386368	-0.045760	4.815611
213.038384	8000.186652	9.391373	-0.045747	4.815632
213.283581	8000.106356	9.396378	-0.045793	4.815607
213.319997	8000.177496	9.401383	-0.045801	4.815628
213.107059	8000.150603	9.406387	-0.045762	4.815621
213.149220	8000.122527	9.411392	-0.045771	4.815613
213.234133	8000.117572	9.416397	-0.045787	4.815611
213.050533	8000.084750	9.421402	-0.045754	4.815602
213.075673	8000.136485	9.426407	-0.045759	4.815617
213.212040	8000.101401	9.431411	-0.045786	4.815606
212.902033	8000.135930	9.436416	-0.045729	4.815618
212.999312	8000.161076	9.441421	-0.045748	4.815625
213.265627	8000.184706	9.446426	-0.045798	4.815630
213.271086	8000.208357	9.451431	-0.045800	4.815637
213.102881	8000.148021	9.456435	-0.045769	4.815620
213.277328	8000.154136	9.461440	-0.045803	4.815621
213.165900	8000.107539	9.466445	-0.045783	4.815608
213.140364	8000.086903	9.471450	-0.045779	4.815602
213.085675	8000.124523	9.476455	-0.045769	4.815613
213.238984	8000.091851	9.481459	-0.045799	4.815603
213.447075	8000.148703	9.486464	-0.045838	4.815619
213.335169	8000.171510	9.491469	-0.045818	4.815626
213.214628	8000.123696	9.496474	-0.045796	4.815612
213.285945	8000.170845	9.501479	-0.045810	4.815626
213.153253	8000.136716	9.506483	-0.045787	4.815616
213.332710	8000.110877	9.511488	-0.045821	4.815608
213.308888	8000.139390	9.516493	-0.045817	4.815616
213.270710	8000.092919	9.521498	-0.045811	4.815603
213.386503	8000.165354	9.526503	-0.045833	4.815624
213.486902	8000.189484	9.531507	-0.045853	4.815630
213.487185	8000.157521	9.536512	-0.045853	4.815621
213.321155	8000.112170	9.541517	-0.045823	4.815608
213.218619	8000.107365	9.546522	-0.045805	4.815607
213.398231	8000.172297	9.551527	-0.045839	4.815626
213.335484	8000.139307	9.556531	-0.045828	4.815616
213.241656	8000.138915	9.561536	-0.045812	4.815616
213.366891	8000.193350	9.566541	-0.045836	4.815632
213.250800	8000.161627	9.571546	-0.045815	4.815623
213.539936	8000.221937	9.576551	-0.045870	4.815639
213.523760	8000.154466	9.581555	-0.045867	4.815620
213.661636	8000.130086	9.586560	-0.045894	4.815612
213.582946	8000.190809	9.591565	-0.045880	4.815630
213.729168	8000.124917	9.596570	-0.045908	4.815610
213.789333	8000.154799	9.601575	-0.045920	4.815618
213.414466	8000.194677	9.606579	-0.045851	4.815632
213.569613	8000.198342	9.611584	-0.045881	4.815632
213.571427	8000.178151	9.616589	-0.045882	4.815626
213.613796	8000.097753	9.621594	-0.045890	4.815602
213.708837	8000.155968	9.626599	-0.045909	4.815619
213.558858	8000.135438	9.631603	-0.045882	4.815614
213.735644	8000.146932	9.636608	-0.045915	4.815616
213.690693	8000.201797	9.641613	-0.045908	4.815632
213.651699	8000.148905	9.646618	-0.045901	4.815617
213.848918	8000.160731	9.651623	-0.045939	4.815620
213.799374	8000.113006	9.656627	-0.045930	4.815606
213.671652	8000.170794	9.661632	-0.045908	4.815623
213.665689	8000.141934	9.666637	-0.045907	4.815615
213.791387	8000.146187	9.671642	-0.045931	4.815616
213.794233	8000.205036	9.676647	-0.045933	4.815633
213.801552	8000.131540	9.681651	-0.045935	4.815611
214.023130	8000.137357	9.686656	-0.045977	4.815612
214.158608	8000.169535	9.691661	-0.046003	4.815621
213.916940	8000.154985	9.696666	-0.045959	4.815617
214.117603	8000.201041	9.701671	-0.045997	4.815630
214.056540	8000.158467	9.706675	-0.045986	4.815618
214.018747	8000.158988	9.711680	-0.045980	4.815618
213.998024	8000.140565	9.716685	-0.045977	4.815613
213.804671	8000.102242	9.721690	-0.045942	4.815602
213.852340	8000.191722	9.726695	-0.045951	4.815628
213.764096	8000.115601	9.731699	-0.045936	4.815606
213.891190	8000.162593	9.736704	-0.045960	4.815620
213.864857	8000.197472	9.741709	-0.045956	4.815630
213.898444	8000.186342	9.746714	-0.045963	4.815626
213.979068	8000.164232	9.751719	-0.045979	4.815620
213.905375	8000.137470	9.756723	-0.045966	4.815612
213.933846	8000.173244	9.761728	-0.045972	4.815622
213.883142	8000.224812	9.766733	-0.045963	4.815638
214.242314	8000.163460	9.771738	-0.046031	4.815618
214.077205	8000.244132	9.776743	-0.046001	4.815642
213.958524	8000.181397	9.781747	-0.045980	4.815625
214.101827	8000.185938	9.786752	-0.046007	4.815625
213.949101	8000.171770	9.791757	-0.045980	4.815622
214.105797	8000.099642	9.796762	-0.046010	4.815600
214.171022	8000.203291	9.801767	-0.046023	4.815630
214.082449	8000.183762	9.806771	-0.046007	4.815625
214.030840	8000.157360	9.811776	-0.045998	4.815617
214.069508	8000.168739	9.816781	-0.046006	4.815620
214.152487	8000.125309	9.821786	-0.046022	4.815607
214.278911	8000.161611	9.826791	-0.046047	4.815617
214.101430	8000.087239	9.831795	-0.046014	4.815596
214.226267	8000.172638	9.836800	-0.046038	4.815621
214.042768	8000.193209	9.841805	-0.046005	4.815627
213.982989	8000.105805	9.846810	-0.045995	4.815602
214.353029	8000.135399	9.851815	-0.046064	4.815609
214.273890	8000.137382	9.856819	-0.046050	4.815610
214.092412	8000.156918	9.861824	-0.046017	4.815616
214.278243	8000.151473	9.866829	-0.046053	4.815614
214.355361	8000.135713	9.871834	-0.046068	4.815609
214.370038	8000.190484	9.876839	-0.046071	4.815625
214.134612	8000.136524	9.881843	-0.046028	4.815610
214.230072	8000.164847	9.886848	-0.046047	4.815618
214.129830	8000.118430	9.891853	-0.046029	4.815605
214.206424	8000.095186	9.896858	-0.046044	4.815598
214.409785	8000.186138	9.901863	-0.046083	4.815623
214.383059	8000.168685	9.906867	-0.046079	4.815618
214.138072	8000.159420	9.911872	-0.046034	4.815617
214.323012	8000.168911	9.916877	-0.046069	4.815619
214.384053	8000.098427	9.921882	-0.046081	4.815598
214.411052	8000.127769	9.926887	-0.046087	4.815606
214.235884	8000.118575	9.931891	-0.046055	4.815604
214.559559	8000.131396	9.936896	-0.046116	4.815606
214.389967	8000.138311	9.941901	-0.046085	4.815609
214.264658	8000.097893	9.946906	-0.046063	4.815598
214.430786	8000.167948	9.951911	-0.046095	4.815618
214.643367	8000.124496	9.956915	-0.046135	4.815604
214.555112	8000.118854	9.961920	-0.046119	4.815603
214.517724	8000.175980	9.966925	-0.046113	4.815620
214.366862	8000.123398	9.971930	-0.046086	4.815605
214.486397	8000.196965	9.976935	-0.046109	4.815626
214.313634	8000.106650	9.981939	-0.046077	4.815600
214.601068	8000.137035	9.986944	-0.046132	4.815608
214.584638	8000.164601	9.991949	-0.046129	4.815616
214.571687	8000.126014	9.996954	-0.046128	4.815605
214.590622	8000.146682	10.001959	-0.046132	4.815611
214.483771	8000.094818	10.006963	-0.046113	4.815596
214.494338	8000.148454	10.011968	-0.046116	4.815611
214.392289	8000.176760	10.016973	-0.046098	4.815620
214.571200	8000.217123	10.021978	-0.046132	4.815631
214.599525	8000.219790	10.026983	-0.046138	4.815632
214.334924	8000.223019	10.031987	-0.046089	4.815634
214.478092	8000.206201	10.036992	-0.046117	4.815628
214.650065	8000.222957	10.041997	-0.046150	4.815632
214.556544	8000.224704	10.047002	-0.046133	4.815633
214.388007	8000.236976	10.052007	-0.046102	4.815638
214.488040	8000.178873	10.057011	-0.046122	4.815620
214.618697	8000.196024	10.062016	-0.046147	4.815625
214.342640	8000.156350	10.067021	-0.046096	4.815614
214.508962	8000.126026	10.072026	-0.046128	4.815605
214.573259	8000.217916	10.077031	-0.046141	4.815631
214.390710	8000.161613	10.082035	-0.046108	4.815616
214.552613	8000.196359	10.087040	-0.046139	4.815625
214.502549	8000.214834	10.092045	-0.046130	4.815631
214.479808	8000.173951	10.097050	-0.046127	4.815619
214.406111	8000.178158	10.102055	-0.046114	4.815620
214.323462	8000.180083	10.107059	-0.046099	4.815621
214.524783	8000.195182	10.112064	-0.046137	4.815625
214.533831	8000.278696	10.117069	-0.046140	4.815649
214.414615	8000.249055	10.122074	-0.046118	4.815641
214.462056	8000.299021	10.127079	-0.046128	4.815655
214.408759	8000.253369	10.132083	-0.046119	4.815642
214.541272	8000.234241	10.137088	-0.046144	4.815636
214.580812	8000.243498	10.142093	-0.046152	4.815638
214.286362	8000.182166	10.147098	-0.046098	4.815622
214.375602	8000.206116	10.152103	-0.046116	4.815628
214.369593	8000.160167	10.157107	-0.046115	4.815615
214.513296	8000.207432	10.162112	-0.046143	4.815628
214.499410	8000.204070	10.167117	-0.046141	4.815627
214.575904	8000.187232	10.172122	-0.046156	4.815622
214.757412	8000.211620	10.177127	-0.046191	4.815628
214.612254	8000.206118	10.182131	-0.046165	4.815627
214.551749	8000.258595	10.187136	-0.046154	4.815643
214.549525	8000.269307	10.192141	-0.046155	4.815646
214.748772	8000.188261	10.197146	-0.046192	4.815621
214.770079	8000.159844	10.202151	-0.046197	4.815613
214.655848	8000.150574	10.207155	-0.046177	4.815611
214.672063	8000.185081	10.212160	-0.046180	4.815621
214.781893	8000.239269	10.217165	-0.046202	4.815636
214.451632	8000.162402	10.222170	-0.046141	4.815615
214.736184	8000.192741	10.227175	-0.046195	4.815622
214.573620	8000.205110	10.232179	-0.046165	4.815627
214.871719	8000.189750	10.237184	-0.046222	4.815621
214.832797	8000.213746	10.242189	-0.046215	4.815628
214.685180	8000.214612	10.247194	-0.046188	4.815629
214.610431	8000.257246	10.252199	-0.046175	4.815642
214.556011	8000.180606	10.257203	-0.046166	4.815620
214.615169	8000.146398	10.262208	-0.046178	4.815609
214.744954	8000.188097	10.267213	-0.046203	4.815621
214.781201	8000.195164	10.272218	-0.046210	4.815623
214.766690	8000.205676	10.277223	-0.046208	4.815626
214.655697	8000.192187	10.282227	-0.046188	4.815622
214.742504	8000.222506	10.287232	-0.046205	4.815631
214.781281	8000.225343	10.292237	-0.046213	4.815631
214.890224	8000.211171	10.297242	-0.046234	4.815627
214.835483	8000.263743	10.302247	-0.046225	4.815642
214.737879	8000.212027	10.307251	-0.046208	4.815628
214.955263	8000.226321	10.312256	-0.046249	4.815631
214.948483	8000.243367	10.317261	-0.046248	4.815636
214.856793	8000.208834	10.322266	-0.046232	4.815626
214.881458	8000.269109	10.327271	-0.046238	4.815644
214.705462	8000.219319	10.332275	-0.046206	4.815630
214.666386	8000.234769	10.337280	-0.046199	4.815635
214.726641	8000.283878	10.342285	-0.046211	4.815649
214.760556	8000.238579	10.347290	-0.046218	4.815635
214.808944	8000.235166	10.352295	-0.046228	4.815634
214.813698	8000.160558	10.357299	-0.046230	4.815612
214.962862	8000.189758	10.362304	-0.046258	4.815620
214.953736	8000.263365	10.367309	-0.046257	4.815641
214.845875	8000.200803	10.372314	-0.046238	4.815624
214.947648	8000.229230	10.377319	-0.046258	4.815631
215.085834	8000.198448	10.382323	-0.046284	4.815622
214.992976	8000.183119	10.387328	-0.046268	4.815618
214.956486	8000.230649	10.392333	-0.046262	4.815632
215.010929	8000.203840	10.397338	-0.046273	4.815624
215.057195	8000.290099	10.402343	-0.046282	4.815649
214.883478	8000.277722	10.407347	-0.046251	4.815646
214.845918	8000.264363	10.412352	-0.046244	4.815642
214.760129	8000.265169	10.417357	-0.046229	4.815643
214.612770	8000.192351	10.422362	-0.046202	4.815622
214.766293	8000.278222	10.427367	-0.046232	4.815646
214.875880	8000.229887	10.432371	-0.046253	4.815632
214.708496	8000.287029	10.437376	-0.046223	4.815649
214.733812	8000.281103	10.442381	-0.046228	4.815647
214.813048	8000.229069	10.447386	-0.046244	4.815632
214.763130	8000.250750	10.452391	-0.046235	4.815638
214.880902	8000.221770	10.457395	-0.046258	4.815629
215.031225	8000.233903	10.462400	-0.046287	4.815632
215.014181	8000.272139	10.467405	-0.046284	4.815643
214.839730	8000.207423	10.472410	-0.046253	4.815625
215.153690	8000.219021	10.477415	-0.046312	4.815627
215.210525	8000.264870	10.482419	-0.046323	4.815640
215.055340	8000.204739	10.487424	-0.046295	4.815623
214.785107	8000.222826	10.492429	-0.046246	4.815630
214.808278	8000.170945	10.497434	-0.046251	4.815615
215.008567	8000.263987	10.502439	-0.046289	4.815641
214.748689	8000.242730	10.507443	-0.046241	4.815636
214.910569	8000.276410	10.512448	-0.046272	4.815645
214.957291	8000.254814	10.517453	-0.046282	4.815638
214.915045	8000.195458	10.522458	-0.046275	4.815621
215.052730	8000.247966	10.527463	-0.046301	4.815636
215.151884	8000.283827	10.532467	-0.046320	4.815646
215.146612	8000.206918	10.537472	-0.046320	4.815623
215.120253	8000.219373	10.542477	-0.046316	4.815627
214.963968	8000.226503	10.547482	-0.046288	4.815630
215.043632	8000.291948	10.552487	-0.046303	4.815649
214.846162	8000.232195	10.557491	-0.046267	4.815632
215.019527	8000.188103	10.562496	-0.046300	4.815618
215.030681	8000.208645	10.567501	-0.046303	4.815624
215.024976	8000.210757	10.572506	-0.046303	4.815625
215.048066	8000.257124	10.577511	-0.046308	4.815638
215.097018	8000.279350	10.582515	-0.046318	4.815645
214.989654	8000.216795	10.587520	-0.046299	4.815627
214.909446	8000.247594	10.592525	-0.046285	4.815636
214.789702	8000.204060	10.597530	-0.046263	4.815624
215.002396	8000.255656	10.602535	-0.046303	4.815638
214.772787	8000.239164	10.607539	-0.046261	4.815634
214.834131	8000.246641	10.612544	-0.046274	4.815636
215.097179	8000.260613	10.617549	-0.046323	4.815639
214.905682	8000.200957	10.622554	-0.046289	4.815622
214.964874	8000.201992	10.627559	-0.046300	4.815622
214.904141	8000.229904	10.632563	-0.046290	4.815631
215.069224	8000.224123	10.637568	-0.046321	4.815628
214.947553	8000.237158	10.642573	-0.046300	4.815633
214.806474	8000.189005	10.647578	-0.046274	4.815619
215.025425	8000.241771	10.652583	-0.046316	4.815634
215.050071	8000.157875	10.657587	-0.046321	4.815609
215.080544	8000.168053	10.662592	-0.046327	4.815612
215.151629	8000.206659	10.667597	-0.046341	4.815623
214.994633	8000.169993	10.672602	-0.046313	4.815613
215.118161	8000.240425	10.677607	-0.046337	4.815633
215.251730	8000.211703	10.682611	-0.046362	4.815624
215.284298	8000.236866	10.687616	-0.046369	4.815631
215.311440	8000.218155	10.692621	-0.046375	4.815625
215.339256	8000.186640	10.697626	-0.046381	4.815616
215.508677	8000.221512	10.702631	-0.046413	4.815625
215.248349	8000.171412	10.707635	-0.046366	4.815612
215.129216	8000.155654	10.712640	-0.046344	4.815608
215.250962	8000.166253	10.717645	-0.046368	4.815610
215.282464	8000.159360	10.722650	-0.046374	4.815608
215.233332	8000.218432	10.727655	-0.046366	4.815626
215.246261	8000.218712	10.732659	-0.046369	4.815626
215.195332	8000.169893	10.737664	-0.046361	4.815611
215.103294	8000.204770	10.742669	-0.046344	4.815622
215.135080	8000.169048	10.747674	-0.046351	4.815611
215.129540	8000.236306	10.752679	-0.046351	4.815631
214.977776	8000.201861	10.757683	-0.046323	4.815622
215.115794	8000.181755	10.762688	-0.046350	4.815615
215.203926	8000.222776	10.767693	-0.046367	4.815627
215.093572	8000.183667	10.772698	-0.046347	4.815616
215.266362	8000.281602	10.777703	-0.046380	4.815644
215.412482	8000.266968	10.782707	-0.046408	4.815639
215.473373	8000.201818	10.787712	-0.046420	4.815619
215.417920	8000.233021	10.792717	-0.046411	4.815629
215.080926	8000.185941	10.797722	-0.046349	4.815616
215.317048	8000.250736	10.802727	-0.046394	4.815634
215.300883	8000.209959	10.807731	-0.046391	4.815622
215.349053	8000.223629	10.812736	-0.046401	4.815626
215.277561	8000.279133	10.817741	-0.046389	4.815643
215.249741	8000.177294	10.822746	-0.046384	4.815613
215.049712	8000.234971	10.827751	-0.046348	4.815631
215.043427	8000.208239	10.832755	-0.046347	4.815623
215.101455	8000.190032	10.837760	-0.046359	4.815617
215.150655	8000.253912	10.842765	-0.046369	4.815636
215.324312	8000.186331	10.847770	-0.046402	4.815615
215.244859	8000.225685	10.852775	-0.046388	4.815627
215.187325	8000.155400	10.857779	-0.046378	4.815607
215.177859	8000.176673	10.862784	-0.046377	4.815613
215.396301	8000.180306	10.867789	-0.046418	4.815613
215.337230	8000.182615	10.872794	-0.046408	4.815614
215.246853	8000.244218	10.877799	-0.046392	4.815632
215.132330	8000.236011	10.882803	-0.046372	4.815631
215.405093	8000.228783	10.887808	-0.046423	4.815627
215.446150	8000.194280	10.892813	-0.046432	4.815617
215.413484	8000.182069	10.897818	-0.046426	4.815613
215.673187	8000.261133	10.902823	-0.046476	4.815635
215.591927	8000.263079	10.907827	-0.046461	4.815636
215.599133	8000.214140	10.912832	-0.046463	4.815622
215.448323	8000.191457	10.917837	-0.046436	4.815616
215.407275	8000.149206	10.922842	-0.046429	4.815604
215.407951	8000.229382	10.927847	-0.046430	4.815627
215.280625	8000.196403	10.932851	-0.046407	4.815618
215.569245	8000.209726	10.937856	-0.046462	4.815621
215.616203	8000.277842	10.942861	-0.046471	4.815640
215.417884	8000.206326	10.947866	-0.046435	4.815620
215.784836	8000.242286	10.952871	-0.046504	4.815629
215.571970	8000.217522	10.957875	-0.046465	4.815623
215.584947	8000.196444	10.962880	-0.046469	4.815616
215.476476	8000.225713	10.967885	-0.046449	4.815626
215.426416	8000.205742	10.972890	-0.046441	4.815620
215.497437	8000.202698	10.977895	-0.046455	4.815619
215.425223	8000.254986	10.982899	-0.046442	4.815634
215.533317	8000.251480	10.987904	-0.046463	4.815633
215.503593	8000.267083	10.992909	-0.046458	4.815637
215.253104	8000.212871	10.997914	-0.046412	4.815623
215.215630	8000.219804	11.002919	-0.046406	4.815625
215.368427	8000.236250	11.007923	-0.046435	4.815629
215.331199	8000.195129	11.012928	-0.046429	4.815617
215.429215	8000.166895	11.017933	-0.046448	4.815608
215.556032	8000.120976	11.022938	-0.046473	4.815594
215.675616	8000.218044	11.027943	-0.046496	4.815622
215.445868	8000.203684	11.032947	-0.046454	4.815619
215.603706	8000.209533	11.037952	-0.046484	4.815620
215.682388	8000.263216	11.042957	-0.046499	4.815635
215.541193	8000.233214	11.047962	-0.046474	4.815627
215.821288	8000.286981	11.052967	-0.046527	4.815641
215.731989	8000.272777	11.057971	-0.046511	4.815638
215.669526	8000.218428	11.062976	-0.046500	4.815622
215.714901	8000.229917	11.067981	-0.046509	4.815625
215.711891	8000.218190	11.072986	-0.046510	4.815622
215.761649	8000.279945	11.077991	-0.046520	4.815640
215.258989	8000.229092	11.082995	-0.046427	4.815627
215.423552	8000.199808	11.088000	-0.046458	4.815618
215.696301	8000.211804	11.093005	-0.046510	4.815620
215.612391	8000.162445	11.098010	-0.046495	4.815606
215.636408	8000.243003	11.103015	-0.046500	4.815629
215.623458	8000.271696	11.108019	-0.046499	4.815638
215.706579	8000.262442	11.113024	-0.046515	4.815635
215.778922	8000.286119	11.118029	-0.046529	4.815641
215.642288	8000.217744	11.123034	-0.046504	4.815622
215.723489	8000.285352	11.128039	-0.046520	4.815641
215.633453	8000.167544	11.133043	-0.046504	4.815607
215.726772	8000.223602	11.138048	-0.046523	4.815623
215.717478	8000.277986	11.143053	-0.046522	4.815639
215.721073	8000.227919	11.148058	-0.046523	4.815624
215.567277	8000.257517	11.153063	-0.046495	4.815634
215.585572	8000.229049	11.158067	-0.046499	4.815625
215.691428	8000.228710	11.163072	-0.046520	4.815625
215.723315	8000.261339	11.168077	-0.046527	4.815634
215.845802	8000.224961	11.173082	-0.046550	4.815623
215.799002	8000.276596	11.178087	-0.046542	4.815638
215.534296	8000.272344	11.183091	-0.046494	4.815638
215.703339	8000.243134	11.188096	-0.046526	4.815629
215.849804	8000.294720	11.193101	-0.046554	4.815643
215.465525	8000.246866	11.198106	-0.046483	4.815631
215.644859	8000.226367	11.203111	-0.046518	4.815624
215.531680	8000.268375	11.208115	-0.046497	4.815637
215.627353	8000.310588	11.213120	-0.046516	4.815649
215.485435	8000.307273	11.218125	-0.046490	4.815648
215.476725	8000.247394	11.223130	-0.046489	4.815631
215.684128	8000.283955	11.228135	-0.046529	4.815641
215.526091	8000.215231	11.233139	-0.046500	4.815621
215.444674	8000.239602	11.238144	-0.046486	4.815629
215.508117	8000.268474	11.243149	-0.046498	4.815637
215.427639	8000.219171	11.248154	-0.046484	4.815623
215.513020	8000.260148	11.253159	-0.046501	4.815634
215.492720	8000.218235	11.258163	-0.046498	4.815622
215.427301	8000.230052	11.263168	-0.046487	4.815626
215.458825	8000.246655	11.268173	-0.046493	4.815631
215.575339	8000.217655	11.273178	-0.046516	4.815621
215.844847	8000.257366	11.278183	-0.046567	4.815632
215.678118	8000.269665	11.283187	-0.046536	4.815636
215.719634	8000.253324	11.288192	-0.046545	4.815631
215.763752	8000.219939	11.293197	-0.046554	4.815621
215.715694	8000.211748	11.298202	-0.046546	4.815619
215.564993	8000.262755	11.303207	-0.046518	4.815635
215.605787	8000.198344	11.308211	-0.046527	4.815616
215.534137	8000.186564	11.313216	-0.046514	4.815612
215.716690	8000.256895	11.318221	-0.046549	4.815632
215.573676	8000.222590	11.323226	-0.046523	4.815623
215.649208	8000.308261	11.328231	-0.046538	4.815647
215.648222	8000.286955	11.333235	-0.046539	4.815641
215.622697	8000.255636	11.338240	-0.046535	4.815632
215.791306	8000.290497	11.343245	-0.046567	4.815641
215.916719	8000.248827	11.348250	-0.046591	4.815629
215.785696	8000.291612	11.353255	-0.046567	4.815642
215.831438	8000.280680	11.358259	-0.046577	4.815638
215.892382	8000.297763	11.363264	-0.046589	4.815643
215.752332	8000.277390	11.368269	-0.046564	4.815638
215.564701	8000.273329	11.373274	-0.046529	4.815637
215.857962	8000.315564	11.378279	-0.046585	4.815648
215.586695	8000.306933	11.383283	-0.046535	4.815647
215.526003	8000.293195	11.388288	-0.046525	4.815643
215.650437	8000.307043	11.393293	-0.046549	4.815647
215.619212	8000.227573	11.398298	-0.046544	4.815624
215.630419	8000.292971	11.403303	-0.046546	4.815643
215.766218	8000.278170	11.408307	-0.046573	4.815638
215.862175	8000.269126	11.413312	-0.046591	4.815635
215.814144	8000.305790	11.418317	-0.046583	4.815646
215.690249	8000.220534	11.423322	-0.046561	4.815621
215.787176	8000.263837	11.428327	-0.046580	4.815633
215.625229	8000.301845	11.433331	-0.046550	4.815645
215.662891	8000.308936	11.438336	-0.046558	4.815647
215.816534	8000.263455	11.443341	-0.046587	4.815633
215.820671	8000.275339	11.448346	-0.046589	4.815636
215.853060	8000.277005	11.453351	-0.046596	4.815637
215.902084	8000.278943	11.458355	-0.046606	4.815637
215.880459	8000.271183	11.463360	-0.046602	4.815635
215.773503	8000.323972	11.468365	-0.046583	4.815651
215.647562	8000.247227	11.473370	-0.046561	4.815629
215.981791	8000.261297	11.478375	-0.046624	4.815631
216.020152	8000.255584	11.483379	-0.046632	4.815630
215.962132	8000.219463	11.488384	-0.046622	4.815619
215.988515	8000.282973	11.493389	-0.046627	4.815638
215.918668	8000.227435	11.498394	-0.046615	4.815622
215.880618	8000.249310	11.503399	-0.046609	4.815628
215.842747	8000.264781	11.508403	-0.046603	4.815633
215.977707	8000.242490	11.513408	-0.046628	4.815626
215.981759	8000.293888	11.518413	-0.046630	4.815641
215.830979	8000.240233	11.523418	-0.046603	4.815626
216.047768	8000.349571	11.528423	-0.046644	4.815657
215.963079	8000.305538	11.533427	-0.046629	4.815644
215.927989	8000.252703	11.538432	-0.046623	4.815629
215.858839	8000.334946	11.543437	-0.046611	4.815653
215.933727	8000.297790	11.548442	-0.046626	4.815642
215.968155	8000.315509	11.553447	-0.046633	4.815647
215.590982	8000.265633	11.558451	-0.046564	4.815634
215.666607	8000.204995	11.563456	-0.046578	4.815616
215.844826	8000.248556	11.568461	-0.046612	4.815628
215.779284	8000.220856	11.573466	-0.046601	4.815620
215.929903	8000.260763	11.578471	-0.046630	4.815631
215.957401	8000.275165	11.583475	-0.046636	4.815635
215.750470	8000.246224	11.588480	-0.046598	4.815628
215.908851	8000.336453	11.593485	-0.046628	4.815653
215.856635	8000.258775	11.598490	-0.046619	4.815631
216.129874	8000.287869	11.603495	-0.046671	4.815638
215.870363	8000.281565	11.608499	-0.046623	4.815637
215.863104	8000.240932	11.613504	-0.046623	4.815626
216.136950	8000.336251	11.618509	-0.046675	4.815652
215.916026	8000.278246	11.623514	-0.046634	4.815636
216.151703	8000.328086	11.628519	-0.046679	4.815650
216.032363	8000.311255	11.633523	-0.046658	4.815645
215.896827	8000.281343	11.638528	-0.046633	4.815637
215.924631	8000.312838	11.643533	-0.046639	4.815646
216.027317	8000.252641	11.648538	-0.046659	4.815628
215.807738	8000.289708	11.653543	-0.046619	4.815640
215.720800	8000.274474	11.658547	-0.046603	4.815636
215.878173	8000.210898	11.663552	-0.046633	4.815616
215.997420	8000.284468	11.668557	-0.046657	4.815637
215.881778	8000.221775	11.673562	-0.046636	4.815620
216.061150	8000.280307	11.678567	-0.046670	4.815636
216.039154	8000.266133	11.683571	-0.046667	4.815632
216.091685	8000.276672	11.688576	-0.046677	4.815635
216.071759	8000.314863	11.693581	-0.046674	4.815646
215.988645	8000.247360	11.698586	-0.046660	4.815626
216.188095	8000.317969	11.703591	-0.046698	4.815646
216.030531	8000.271678	11.708595	-0.046669	4.815633
216.037299	8000.265450	11.713600	-0.046671	4.815631
216.121075	8000.286110	11.718605	-0.046687	4.815637
215.865216	8000.224331	11.723610	-0.046641	4.815620
215.791572	8000.236013	11.728615	-0.046628	4.815624
215.946637	8000.263178	11.733619	-0.046657	4.815631
216.008223	8000.186290	11.738624	-0.046669	4.815608
215.961977	8000.319101	11.743629	-0.046662	4.815647
215.950340	8000.286941	11.748634	-0.046660	4.815638
216.000876	8000.320943	11.753639	-0.046671	4.815648
216.033048	8000.302313	11.758643	-0.046677	4.815642
216.191511	8000.346622	11.763648	-0.046708	4.815654
216.283999	8000.340726	11.768653	-0.046726	4.815652
215.980350	8000.250397	11.773658	-0.046670	4.815627
216.122489	8000.310458	11.778663	-0.046697	4.815644
216.085306	8000.293900	11.783667	-0.046691	4.815639
216.099945	8000.277121	11.788672	-0.046695	4.815634
216.074012	8000.309874	11.793677	-0.046690	4.815644
216.266348	8000.294928	11.798682	-0.046727	4.815639
216.413191	8000.320891	11.803687	-0.046755	4.815646
216.254204	8000.314092	11.808691	-0.046726	4.815644
216.034650	8000.268924	11.813696	-0.046686	4.815632
216.043208	8000.305444	11.818701	-0.046689	4.815643
216.053161	8000.265092	11.823706	-0.046691	4.815631
215.988067	8000.288662	11.828711	-0.046680	4.815638
216.125277	8000.245049	11.833715	-0.046706	4.815625
216.171966	8000.240540	11.838720	-0.046716	4.815623
216.226967	8000.308791	11.843725	-0.046727	4.815643
216.092377	8000.285302	11.848730	-0.046703	4.815636
216.253418	8000.296545	11.853735	-0.046733	4.815639
216.084196	8000.294918	11.858739	-0.046703	4.815639
216.235451	8000.250466	11.863744	-0.046732	4.815626
216.211143	8000.335578	11.868749	-0.046728	4.815651
216.143770	8000.299303	11.873754	-0.046716	4.815640
216.244836	8000.320246	11.878759	-0.046736	4.815646
216.075292	8000.313274	11.883763	-0.046705	4.815645
216.250084	8000.325810	11.888768	-0.046738	4.815647
216.086535	8000.312528	11.893773	-0.046709	4.815644
215.976548	8000.288373	11.898778	-0.046689	4.815638
216.183011	8000.301426	11.903783	-0.046728	4.815641
216.083177	8000.280641	11.908787	-0.046710	4.815635
215.999877	8000.274010	11.913792	-0.046696	4.815633
216.010545	8000.321244	11.918797	-0.046698	4.815647
215.921343	8000.264322	11.923802	-0.046683	4.815631
216.045776	8000.352930	11.928807	-0.046707	4.815656
216.052556	8000.358450	11.933811	-0.046709	4.815658
216.021294	8000.289657	11.938816	-0.046704	4.815638
216.306228	8000.368071	11.943821	-0.046757	4.815659
216.040620	8000.299722	11.948826	-0.046709	4.815641
216.326011	8000.345036	11.953831	-0.046763	4.815652
216.202940	8000.316395	11.958835	-0.046740	4.815645
216.135481	8000.304683	11.963840	-0.046729	4.815641
216.079673	8000.355104	11.968845	-0.046719	4.815656
216.340034	8000.343406	11.973850	-0.046768	4.815652
216.296931	8000.356655	11.978855	-0.046761	4.815656
216.132376	8000.316656	11.983859	-0.046731	4.815645
215.986001	8000.276955	11.988864	-0.046705	4.815634
216.111198	8000.342081	11.993869	-0.046729	4.815652
216.104883	8000.308939	11.998874	-0.046729	4.815643
216.321705	8000.333909	12.003879	-0.046770	4.815649
216.281825	8000.332259	12.008883	-0.046763	4.815649
216.000480	8000.268993	12.013888	-0.046711	4.815631
216.379625	8000.316907	12.018893	-0.046783	4.815644
216.278526	8000.320664	12.023898	-0.046765	4.815645
216.307375	8000.345769	12.028903	-0.046771	4.815652
216.296786	8000.321101	12.033907	-0.046770	4.815645
216.539602	8000.239696	12.038912	-0.046816	4.815620
216.455023	8000.321688	12.043917	-0.046801	4.815645
216.302024	8000.340618	12.048922	-0.046773	4.815651
216.420073	8000.322323	12.053927	-0.046796	4.815645
216.179659	8000.338757	12.058931	-0.046752	4.815651
216.373286	8000.336649	12.063936	-0.046789	4.815649
216.302298	8000.360122	12.068941	-0.046776	4.815656
216.256961	8000.330615	12.073946	-0.046769	4.815648
216.273632	8000.384356	12.078951	-0.046773	4.815664
216.282851	8000.321564	12.083955	-0.046775	4.815645
216.434889	8000.323049	12.088960	-0.046804	4.815645
216.482105	8000.369813	12.093965	-0.046814	4.815658
216.371691	8000.325359	12.098970	-0.046794	4.815646
216.508299	8000.356495	12.103975	-0.046820	4.815654
216.278873	8000.369905	12.108979	-0.046778	4.815659
216.305969	8000.281772	12.113984	-0.046784	4.815633
216.495562	8000.316978	12.118989	-0.046820	4.815643
216.377977	8000.255319	12.123994	-0.046799	4.815625
216.439101	8000.325806	12.128999	-0.046811	4.815646
216.203039	8000.303864	12.134003	-0.046768	4.815640
216.294281	8000.234935	12.139008	-0.046786	4.815620
216.323964	8000.350833	12.144013	-0.046792	4.815653
216.188656	8000.233348	12.149018	-0.046768	4.815620
216.322101	8000.232393	12.154023	-0.046793	4.815619
216.382947	8000.299672	12.159027	-0.046806	4.815638
216.445956	8000.220670	12.164032	-0.046818	4.815615
216.490766	8000.288755	12.169037	-0.046827	4.815634
216.592184	8000.284073	12.174042	-0.046847	4.815632
216.659175	8000.377085	12.179047	-0.046860	4.815659
216.527643	8000.340829	12.184051	-0.046836	4.815649
216.514329	8000.316117	12.189056	-0.046835	4.815642
216.640743	8000.363107	12.194061	-0.046859	4.815655
216.486105	8000.318998	12.199066	-0.046831	4.815643
216.554417	8000.341543	12.204071	-0.046845	4.815649
216.382452	8000.345211	12.209075	-0.046813	4.815651
216.336003	8000.326365	12.214080	-0.046805	4.815646
216.148252	8000.304143	12.219085	-0.046771	4.815640
216.293617	8000.258527	12.224090	-0.046799	4.815626
216.428963	8000.298187	12.229095	-0.046825	4.815637
216.408049	8000.244514	12.234099	-0.046822	4.815621
216.460381	8000.296702	12.239104	-0.046833	4.815636
216.543678	8000.349396	12.244109	-0.046849	4.815651
216.336407	8000.253163	12.249114	-0.046811	4.815624
216.376247	8000.281651	12.254119	-0.046819	4.815632
216.579166	8000.319211	12.259123	-0.046858	4.815642
216.455107	8000.310846	12.264128	-0.046836	4.815641
216.471071	8000.327196	12.269133	-0.046839	4.815645
216.519773	8000.323788	12.274138	-0.046849	4.815644
216.768012	8000.309757	12.279143	-0.046896	4.815639
216.639770	8000.291711	12.284147	-0.046873	4.815634
216.598122	8000.293235	12.289152	-0.046866	4.815635
216.741904	8000.340510	12.294157	-0.046894	4.815648
216.536688	8000.323342	12.299162	-0.046856	4.815644
216.482960	8000.385546	12.304167	-0.046847	4.815662
216.453019	8000.350950	12.309171	-0.046842	4.815652
216.416866	8000.339748	12.314176	-0.046836	4.815649
216.323925	8000.355387	12.319181	-0.046820	4.815654
216.391227	8000.270047	12.324186	-0.046833	4.815629
216.416240	8000.365578	12.329191	-0.046839	4.815656
216.365633	8000.329576	12.334195	-0.046830	4.815646
216.398872	8000.343004	12.339200	-0.046837	4.815650
216.506502	8000.352307	12.344205	-0.046858	4.815652
216.485276	8000.260181	12.349210	-0.046854	4.815625
216.669828	8000.298509	12.354215	-0.046890	4.815636
216.492283	8000.354419	12.359219	-0.046857	4.815653
216.597016	8000.330566	12.364224	-0.046878	4.815645
216.708243	8000.360221	12.369229	-0.046899	4.815653
216.668998	8000.348969	12.374234	-0.046893	4.815650
216.590593	8000.350961	12.379239	-0.046879	4.815651
216.479655	8000.291545	12.384243	-0.046859	4.815634
216.572693	8000.278182	12.389248	-0.046877	4.815630
216.619090	8000.364450	12.394253	-0.046887	4.815655
216.332578	8000.303234	12.399258	-0.046834	4.815638
216.487897	8000.325065	12.404263	-0.046864	4.815644
216.438443	8000.363842	12.409267	-0.046855	4.815656
216.515565	8000.287206	12.414272	-0.046870	4.815633
216.549612	8000.354049	12.419277	-0.046878	4.815652
216.682473	8000.302888	12.424282	-0.046903	4.815636
216.709956	8000.321562	12.429287	-0.046909	4.815642
216.610372	8000.348841	12.434291	-0.046891	4.815650
216.418875	8000.289177	12.439296	-0.046856	4.815634
216.539806	8000.360642	12.444301	-0.046880	4.815654
216.487003	8000.375869	12.449306	-0.046871	4.815659
216.507873	8000.352782	12.454311	-0.046875	4.815652
216.559344	8000.336604	12.459315	-0.046886	4.815647
216.603035	8000.297871	12.464320	-0.046895	4.815635
216.582716	8000.418294	12.469325	-0.046892	4.815670
216.448964	8000.327532	12.474330	-0.046867	4.815645
216.627737	8000.310230	12.479335	-0.046902	4.815639
216.807588	8000.381591	12.484339	-0.046936	4.815659
216.682014	8000.289895	12.489344	-0.046913	4.815632
216.681660	8000.282482	12.494349	-0.046914	4.815630
216.579304	8000.256314	12.499354	-0.046896	4.815623
216.500307	8000.284997	12.504359	-0.046882	4.815632
216.660889	8000.345363	12.509363	-0.046912	4.815649
216.655749	8000.335736	12.514368	-0.046912	4.815646
216.567191	8000.379215	12.519373	-0.046897	4.815659
216.491828	8000.350284	12.524378	-0.046883	4.815651
216.817345	8000.346060	12.529383	-0.046945	4.815648
216.742910	8000.358797	12.534387	-0.046932	4.815652
216.482617	8000.269172	12.539392	-0.046884	4.815627
216.530346	8000.349054	12.544397	-0.046894	4.815650
216.429928	8000.330394	12.549402	-0.046876	4.815645
216.442950	8000.266595	12.554407	-0.046879	4.815626
216.487935	8000.269535	12.559411	-0.046888	4.815627
216.488420	8000.209804	12.564416	-0.046889	4.815610
216.543230	8000.272713	12.569421	-0.046900	4.815628
216.715794	8000.255309	12.574426	-0.046933	4.815622
216.698930	8000.324524	12.579431	-0.046931	4.815642
216.661949	8000.325057	12.584435	-0.046924	4.815642
216.410896	8000.237719	12.589440	-0.046878	4.815618
216.689407	8000.257290	12.594445	-0.046931	4.815622
216.565442	8000.214750	12.599450	-0.046909	4.815611
216.660236	8000.283652	12.604455	-0.046927	4.815630
216.586041	8000.332706	12.609459	-0.046914	4.815645
216.826706	8000.267286	12.614464	-0.046960	4.815625
216.752530	8000.333429	12.619469	-0.046947	4.815644
216.555045	8000.285414	12.624474	-0.046911	4.815631
216.718112	8000.294556	12.629479	-0.046942	4.815633
216.641181	8000.331817	12.634483	-0.046928	4.815644
216.577255	8000.298801	12.639488	-0.046917	4.815635
216.696113	8000.363825	12.644493	-0.046940	4.815653
216.759530	8000.347842	12.649498	-0.046953	4.815648
216.703179	8000.306406	12.654503	-0.046943	4.815636
216.548736	8000.356284	12.659507	-0.046915	4.815652
216.715765	8000.333450	12.664512	-0.046947	4.815644
216.813369	8000.303073	12.669517	-0.046966	4.815635
216.773851	8000.309973	12.674522	-0.046959	4.815637
216.983087	8000.316665	12.679527	-0.046999	4.815638
216.870129	8000.288188	12.684531	-0.046979	4.815630
216.775725	8000.272830	12.689536	-0.046962	4.815626
216.937859	8000.346039	12.694541	-0.046993	4.815647
216.878484	8000.315233	12.699546	-0.046983	4.815638
216.918406	8000.290321	12.704551	-0.046991	4.815631
216.759192	8000.363619	12.709555	-0.046962	4.815653
216.767663	8000.320037	12.714560	-0.046965	4.815640
216.725357	8000.285238	12.719565	-0.046957	4.815630
216.776088	8000.338470	12.724570	-0.046968	4.815645
216.672246	8000.399855	12.729575	-0.046949	4.815664
216.799942	8000.387059	12.734579	-0.046974	4.815659
216.746192	8000.336052	12.739584	-0.046965	4.815645
216.824212	8000.376914	12.744589	-0.046980	4.815656
216.772610	8000.325942	12.749594	-0.046971	4.815641
216.755569	8000.288352	12.754599	-0.046969	4.815631
216.685604	8000.341747	12.759603	-0.046956	4.815646
216.624279	8000.306637	12.764608	-0.046946	4.815636
216.790623	8000.314765	12.769613	-0.046978	4.815638
216.611027	8000.268110	12.774618	-0.046945	4.815625
216.827075	8000.312295	12.779623	-0.046986	4.815637
216.850164	8000.291380	12.784627	-0.046991	4.815631
216.771987	8000.265608	12.789632	-0.046977	4.815624
216.851845	8000.342812	12.794637	-0.046993	4.815646
216.844545	8000.321401	12.799642	-0.046992	4.815640
216.783116	8000.361051	12.804647	-0.046982	4.815651
216.746061	8000.405372	12.809651	-0.046976	4.815665
216.683890	8000.357432	12.814656	-0.046965	4.815651
216.766985	8000.385560	12.819661	-0.046981	4.815659
216.725978	8000.324081	12.824666	-0.046974	4.815641
216.755844	8000.327842	12.829671	-0.046981	4.815642
216.779652	8000.326164	12.834675	-0.046986	4.815641
216.803710	8000.297790	12.839680	-0.046991	4.815633
216.781669	8000.348764	12.844685	-0.046988	4.815648
216.728738	8000.265730	12.849690	-0.046979	4.815624
217.008478	8000.286391	12.854695	-0.047031	4.815628
216.728365	8000.320332	12.859699	-0.046980	4.815640
216.679630	8000.303584	12.864704	-0.046972	4.815635
216.886886	8000.351898	12.869709	-0.047011	4.815648
216.493146	8000.245138	12.874714	-0.046939	4.815619
216.772986	8000.259392	12.879719	-0.046992	4.815621
216.839663	8000.359877	12.884723	-0.047005	4.815651
216.705814	8000.311834	12.889728	-0.046981	4.815637
216.779052	8000.289603	12.894733	-0.046995	4.815630
216.752221	8000.287098	12.899738	-0.046991	4.815630
216.858511	8000.304924	12.904743	-0.047011	4.815634
216.522550	8000.381741	12.909747	-0.046950	4.815658
216.634498	8000.317422	12.914752	-0.046971	4.815639
216.894302	8000.307853	12.919757	-0.047020	4.815635
216.700279	8000.273778	12.924762	-0.046985	4.815626
216.865942	8000.296847	12.929767	-0.047017	4.815632
216.771954	8000.319945	12.934771	-0.047000	4.815639
216.899786	8000.321035	12.939776	-0.047025	4.815639
216.736757	8000.331257	12.944781	-0.046995	4.815642
216.750325	8000.298439	12.949786	-0.046998	4.815633
216.832945	8000.387436	12.954791	-0.047015	4.815658
216.749409	8000.358371	12.959795	-0.047000	4.815650
216.596006	8000.298260	12.964800	-0.046972	4.815633
216.802881	8000.358316	12.969805	-0.047011	4.815650
216.676034	8000.308250	12.974810	-0.046988	4.815636
216.498523	8000.309691	12.979815	-0.046956	4.815637
216.683520	8000.325599	12.984819	-0.046991	4.815641
216.885140	8000.255269	12.989824	-0.047030	4.815619
216.869622	8000.336255	12.994829	-0.047028	4.815643
216.859509	8000.325479	12.999834	-0.047027	4.815640
216.980255	8000.269848	13.004839	-0.047050	4.815623
216.940427	8000.328008	13.009843	-0.047043	4.815640
216.836043	8000.312486	13.014848	-0.047025	4.815636
217.089937	8000.336998	13.019853	-0.047073	4.815642
217.022392	8000.282561	13.024858	-0.047061	4.815626
216.896605	8000.274166	13.029863	-0.047038	4.815625
216.974329	8000.347064	13.034867	-0.047054	4.815646
217.099353	8000.251985	13.039872	-0.047078	4.815617
216.996544	8000.310184	13.044877	-0.047059	4.815635
216.842120	8000.279961	13.049882	-0.047031	4.815626
217.009471	8000.337235	13.054887	-0.047063	4.815642
217.068199	8000.358557	13.059891	-0.047075	4.815648
216.819859	8000.311845	13.064896	-0.047029	4.815636
216.929252	8000.356424	13.069901	-0.047051	4.815648
217.017877	8000.278907	13.074906	-0.047068	4.815625
217.119153	8000.269951	13.079911	-0.047088	4.815622
216.864046	8000.322456	13.084915	-0.047041	4.815639
216.826130	8000.313362	13.089920	-0.047035	4.815636
216.977019	8000.321237	13.094925	-0.047063	4.815638
216.896465	8000.270860	13.099930	-0.047049	4.815623
217.103677	8000.264703	13.104935	-0.047089	4.815621
216.968702	8000.306356	13.109939	-0.047064	4.815633
216.894855	8000.315898	13.114944	-0.047051	4.815636
217.023308	8000.319135	13.119949	-0.047076	4.815637
216.917905	8000.265148	13.124954	-0.047057	4.815621
216.867239	8000.350900	13.129959	-0.047049	4.815647
216.844087	8000.367679	13.134963	-0.047045	4.815652
216.819920	8000.329972	13.139968	-0.047041	4.815641
216.996717	8000.345747	13.144973	-0.047075	4.815645
216.791231	8000.338186	13.149978	-0.047038	4.815643
216.992466	8000.295618	13.154983	-0.047076	4.815630
217.026416	8000.360325	13.159987	-0.047083	4.815649
216.874199	8000.320524	13.164992	-0.047055	4.815638
216.982716	8000.345864	13.169997	-0.047076	4.815645
216.899098	8000.280484	13.175002	-0.047062	4.815626
217.097421	8000.291271	13.180007	-0.047099	4.815628
216.933203	8000.319629	13.185011	-0.047069	4.815637
216.700363	8000.230451	13.190016	-0.047027	4.815612
216.884107	8000.305081	13.195021	-0.047062	4.815633
216.777401	8000.248936	13.200026	-0.047043	4.815617
216.881929	8000.351109	13.205031	-0.047063	4.815646
217.010146	8000.331913	13.210035	-0.047088	4.815640
216.614007	8000.341528	13.215040	-0.047015	4.815645
216.743695	8000.366146	13.220045	-0.047040	4.815651
216.711093	8000.358206	13.225050	-0.047034	4.815649
216.792163	8000.343579	13.230055	-0.047050	4.815645
216.613975	8000.396274	13.235059	-0.047018	4.815661
216.695501	8000.296212	13.240064	-0.047034	4.815631
216.871782	8000.354701	13.245069	-0.047068	4.815647
216.811400	8000.319606	13.250074	-0.047057	4.815637
216.935455	8000.321702	13.255079	-0.047081	4.815637
217.078294	8000.324106	13.260083	-0.047108	4.815637
216.797421	8000.305700	13.265088	-0.047057	4.815633
216.826142	8000.359640	13.270093	-0.047063	4.815649
216.740896	8000.340160	13.275098	-0.047048	4.815644
216.849421	8000.355887	13.280103	-0.047069	4.815648
216.731589	8000.372187	13.285107	-0.047048	4.815653
216.640703	8000.294940	13.290112	-0.047032	4.815631
216.980355	8000.376392	13.295117	-0.047096	4.815653
216.709006	8000.301535	13.300122	-0.047046	4.815632
216.754763	8000.323713	13.305127	-0.047055	4.815639
216.793353	8000.350045	13.310131	-0.047063	4.815646
216.904467	8000.381836	13.315136	-0.047085	4.815655
216.848887	8000.404494	13.320141	-0.047075	4.815662
216.775463	8000.353165	13.325146	-0.047062	4.815647
216.821819	8000.331563	13.330151	-0.047072	4.815641
216.873447	8000.382674	13.335155	-0.047082	4.815655
216.777584	8000.297869	13.340160	-0.047065	4.815631
217.032470	8000.375799	13.345165	-0.047113	4.815652
216.907798	8000.363150	13.350170	-0.047091	4.815649
216.897658	8000.322467	13.355175	-0.047090	4.815637
216.908011	8000.324842	13.360179	-0.047092	4.815638
216.710572	8000.301391	13.365184	-0.047056	4.815632
216.882478	8000.374761	13.370189	-0.047089	4.815653
216.802051	8000.250691	13.375194	-0.047075	4.815617
216.885479	8000.236103	13.380199	-0.047091	4.815612
216.856837	8000.309399	13.385203	-0.047087	4.815634
216.751239	8000.288517	13.390208	-0.047068	4.815628
217.060218	8000.308589	13.395213	-0.047126	4.815632
216.979321	8000.304132	13.400218	-0.047112	4.815631
216.949706	8000.326146	13.405223	-0.047107	4.815638
216.836036	8000.388440	13.410227	-0.047087	4.815657
216.942521	8000.373161	13.415232	-0.047107	4.815652
216.782528	8000.399452	13.420237	-0.047078	4.815660
216.792862	8000.324927	13.425242	-0.047081	4.815638
216.863293	8000.311195	13.430247	-0.047095	4.815634
216.849302	8000.367641	13.435251	-0.047093	4.815651
216.776720	8000.285353	13.440256	-0.047080	4.815627
217.038080	8000.317463	13.445261	-0.047130	4.815635
216.939493	8000.307377	13.450266	-0.047112	4.815632
216.907939	8000.359264	13.455271	-0.047107	4.815648
216.872777	8000.371575	13.460275	-0.047102	4.815651
216.990657	8000.281719	13.465280	-0.047124	4.815625
217.105963	8000.365913	13.470285	-0.047147	4.815649
216.875729	8000.318428	13.475290	-0.047104	4.815636
216.937675	8000.310966	13.480295	-0.047117	4.815633
216.881440	8000.341089	13.485299	-0.047107	4.815642
216.724246	8000.301207	13.490304	-0.047079	4.815631
217.082292	8000.337034	13.495309	-0.047146	4.815640
217.057354	8000.302518	13.500314	-0.047142	4.815630
216.938603	8000.319871	13.505319	-0.047121	4.815636
217.157565	8000.384399	13.510323	-0.047162	4.815654
217.099747	8000.298079	13.515328	-0.047152	4.815629
217.109221	8000.364522	13.520333	-0.047155	4.815648
217.143990	8000.359819	13.525338	-0.047162	4.815646
217.185062	8000.343471	13.530343	-0.047171	4.815641
216.950003	8000.379215	13.535347	-0.047128	4.815653
217.014734	8000.317328	13.540352	-0.047141	4.815635
216.965352	8000.410578	13.545357	-0.047132	4.815662
216.890505	8000.316503	13.550362	-0.047119	4.815635
216.908393	8000.396968	13.555367	-0.047123	4.815658
216.946923	8000.388055	13.560371	-0.047131	4.815656
216.917165	8000.323555	13.565376	-0.047126	4.815637
217.009537	8000.380673	13.570381	-0.047144	4.815653
216.907136	8000.352366	13.575386	-0.047126	4.815645
217.100991	8000.329971	13.580391	-0.047163	4.815638
216.852434	8000.337726	13.585395	-0.047117	4.815641
216.956051	8000.243365	13.590400	-0.047137	4.815613
217.146999	8000.333067	13.595405	-0.047174	4.815638
217.028363	8000.317312	13.600410	-0.047153	4.815634
217.108568	8000.310148	13.605415	-0.047168	4.815632
217.244577	8000.370116	13.610419	-0.047194	4.815649
217.086043	8000.271468	13.615424	-0.047166	4.815621
217.130127	8000.337409	13.620429	-0.047175	4.815640
217.000941	8000.289441	13.625434	-0.047151	4.815626
217.015673	8000.275866	13.630439	-0.047155	4.815622
216.895178	8000.304939	13.635443	-0.047133	4.815631
216.896886	8000.284743	13.640448	-0.047134	4.815625
216.979184	8000.375874	13.645453	-0.047151	4.815651
216.854298	8000.311954	13.650458	-0.047128	4.815633
216.847141	8000.332199	13.655463	-0.047128	4.815639
216.900282	8000.363042	13.660467	-0.047138	4.815648
216.872938	8000.342372	13.665472	-0.047134	4.815642
217.013048	8000.308418	13.670477	-0.047161	4.815631
216.989282	8000.335868	13.675482	-0.047157	4.815640
217.286948	8000.332259	13.680487	-0.047213	4.815637
217.110058	8000.343321	13.685491	-0.047181	4.815641
217.074821	8000.302228	13.690496	-0.047175	4.815629
217.100564	8000.376414	13.695501	-0.047181	4.815651
216.917472	8000.340380	13.700506	-0.047148	4.815641
216.920749	8000.313801	13.705511	-0.047149	4.815633
216.897836	8000.322040	13.710515	-0.047146	4.815636
217.022543	8000.280358	13.715520	-0.047170	4.815623
217.009997	8000.328284	13.720525	-0.047168	4.815637
216.871481	8000.363471	13.725530	-0.047143	4.815648
216.871783	8000.378498	13.730535	-0.047144	4.815652
216.734577	8000.353895	13.735539	-0.047119	4.815646
216.803884	8000.294218	13.740544	-0.047133	4.815628
217.103290	8000.347244	13.745549	-0.047189	4.815642
217.177508	8000.336778	13.750554	-0.047204	4.815639
217.170560	8000.289739	13.755559	-0.047203	4.815625
216.883254	8000.342786	13.760563	-0.047151	4.815642
216.998403	8000.277451	13.765568	-0.047173	4.815622
217.153512	8000.299281	13.770573	-0.047203	4.815628
217.125926	8000.325600	13.775578	-0.047198	4.815636
217.059287	8000.304287	13.780583	-0.047187	4.815630
216.930083	8000.373803	13.785587	-0.047163	4.815651
216.811548	8000.366594	13.790592	-0.047142	4.815649
216.839068	8000.367113	13.795597	-0.047148	4.815649
216.829235	8000.373430	13.800602	-0.047147	4.815651
217.024628	8000.338244	13.805607	-0.047184	4.815640
216.955085	8000.368150	13.810611	-0.047172	4.815649
217.092545	8000.312791	13.815616	-0.047198	4.815632
217.008568	8000.312555	13.820621	-0.047184	4.815632
217.084481	8000.304253	13.825626	-0.047198	4.815629
217.038092	8000.298224	13.830631	-0.047191	4.815628
217.000397	8000.285928	13.835635	-0.047184	4.815624
217.019672	8000.284176	13.840640	-0.047189	4.815624
217.025449	8000.359104	13.845645	-0.047191	4.815646
216.938002	8000.294728	13.850650	-0.047175	4.815627
216.956754	8000.300444	13.855655	-0.047179	4.815629
216.677225	8000.399544	13.860659	-0.047128	4.815659
216.846458	8000.345773	13.865664	-0.047160	4.815642
216.988140	8000.334274	13.870669	-0.047188	4.815638
216.715830	8000.249788	13.875674	-0.047138	4.815615
216.850734	8000.236042	13.880679	-0.047164	4.815610
217.186793	8000.340934	13.885683	-0.047227	4.815639
216.985974	8000.242663	13.890688	-0.047190	4.815611
217.070655	8000.281498	13.895693	-0.047207	4.815622
217.171523	8000.246903	13.900698	-0.047226	4.815612
217.138906	8000.295569	13.905703	-0.047221	4.815626
217.062073	8000.282633	13.910707	-0.047208	4.815623
216.979847	8000.261065	13.915712	-0.047193	4.815617
217.208364	8000.290504	13.920717	-0.047236	4.815624
216.957004	8000.260830	13.925722	-0.047190	4.815617
217.025795	8000.281249	13.930727	-0.047204	4.815622
217.246506	8000.385325	13.935731	-0.047246	4.815652
217.097878	8000.293246	13.940736	-0.047219	4.815626
217.005473	8000.358024	13.945741	-0.047203	4.815645
217.029206	8000.370230	13.950746	-0.047208	4.815648
216.980668	8000.274449	13.955751	-0.047200	4.815621
216.912709	8000.390893	13.960755	-0.047188	4.815655
217.008187	8000.331644	13.965760	-0.047206	4.815637
216.978845	8000.342982	13.970765	-0.047202	4.815641
216.901461	8000.307608	13.975770	-0.047188	4.815631
216.822162	8000.355511	13.980775	-0.047174	4.815645
216.966857	8000.381444	13.985779	-0.047202	4.815652
216.968041	8000.361239	13.990784	-0.047203	4.815646
216.969395	8000.382691	13.995789	-0.047204	4.815652
217.092952	8000.384781	14.000794	-0.047228	4.815652
217.096805	8000.298400	14.005799	-0.047229	4.815627
217.183683	8000.345817	14.010803	-0.047246	4.815640
217.198310	8000.235047	14.015808	-0.047250	4.815608
217.238689	8000.311608	14.020813	-0.047258	4.815630
217.012961	8000.309055	14.025818	-0.047217	4.815630
217.111239	8000.303254	14.030823	-0.047236	4.815628
217.242603	8000.357807	14.035827	-0.047261	4.815643
217.155568	8000.310526	14.040832	-0.047246	4.815630
216.999089	8000.403094	14.045837	-0.047217	4.815658
217.234219	8000.377102	14.050842	-0.047262	4.815649
217.149309	8000.313835	14.055847	-0.047247	4.815631
217.038952	8000.395409	14.060851	-0.047227	4.815655
216.893681	8000.332223	14.065856	-0.047201	4.815637
217.267175	7999.345128	14.070861	-0.047270	4.815347

217.020807	7996.077704	14.075866	-0.047223	4.814393
216.954732	7990.565735	14.080871	-0.047208	4.812781
216.892029	7983.963050	14.085875	-0.047193	4.810850
216.941638	7976.604372	14.090880	-0.047198	4.808696
216.891327	7969.043810	14.095885	-0.047185	4.806483
216.746918	7961.211468	14.100890	-0.047153	4.804189
216.895888	7953.384195	14.105895	-0.047177	4.801894
216.883225	7945.388933	14.110899	-0.047170	4.799550
216.587506	7937.471062	14.115904	-0.047111	4.797229
216.624492	7929.422701	14.120909	-0.047113	4.794866
216.617292	7921.393605	14.125914	-0.047107	4.792508
216.539451	7913.360027	14.130919	-0.047088	4.790148
216.790123	7905.405144	14.135923	-0.047131	4.787809
216.550731	7897.389957	14.140928	-0.047082	4.785453
216.542497	7889.431832	14.145933	-0.047076	4.783111
216.538775	7881.411938	14.150938	-0.047071	4.780751
216.342207	7873.392392	14.155943	-0.047030	4.778389
216.445063	7865.461313	14.160947	-0.047044	4.776052
216.164319	7857.381978	14.165952	-0.046988	4.773671
216.496451	7849.319860	14.170957	-0.047045	4.771292
216.404176	7841.315566	14.175962	-0.047023	4.768930
216.224807	7833.359665	14.180967	-0.046986	4.766582
216.054525	7825.397304	14.185971	-0.046949	4.764230
216.010278	7817.428831	14.190976	-0.046937	4.761875
216.068452	7809.389525	14.195981	-0.046943	4.759498
215.931170	7801.362517	14.200986	-0.046913	4.757124
215.831828	7793.371641	14.205991	-0.046890	4.754759
215.922524	7785.352123	14.210995	-0.046903	4.752383
215.643969	7777.253535	14.216000	-0.046846	4.749985
215.827439	7769.382073	14.221005	-0.046876	4.747651
215.701695	7761.299622	14.226010	-0.046848	4.745254
215.713901	7753.377363	14.231015	-0.046846	4.742903
215.709346	7745.348474	14.236019	-0.046841	4.740520
215.469723	7737.331793	14.241024	-0.046792	4.738139
215.726664	7729.352459	14.246029	-0.046835	4.735767
215.522115	7721.300170	14.251034	-0.046793	4.733373
215.545400	7713.296151	14.256039	-0.046793	4.730992
215.342442	7705.298270	14.261043	-0.046750	4.728612
215.215246	7697.286318	14.266048	-0.046722	4.726227
215.579971	7689.358233	14.271053	-0.046786	4.723864
215.653280	7681.328854	14.276058	-0.046795	4.721470
215.256879	7673.314216	14.281063	-0.046717	4.719081
215.185799	7665.384928	14.286067	-0.046699	4.716715
215.430119	7657.313730	14.291072	-0.046740	4.714305
215.346805	7649.331778	14.296077	-0.046720	4.711921
215.231591	7641.309793	14.301082	-0.046694	4.709524
215.268413	7633.293079	14.306087	-0.046697	4.707127
215.293669	7625.294964	14.311091	-0.046697	4.704734
215.175250	7617.297813	14.316096	-0.046671	4.702341
215.100799	7609.306130	14.321101	-0.046652	4.699948
215.105536	7601.302415	14.326106	-0.046649	4.697550
214.896643	7593.278497	14.331111	-0.046605	4.695145
214.944769	7585.303066	14.336115	-0.046610	4.692753
214.802258	7577.243153	14.341120	-0.046579	4.690334
214.741417	7569.307496	14.346125	-0.046563	4.687952
214.709857	7561.239952	14.351130	-0.046553	4.685529
214.758279	7553.299591	14.356135	-0.046558	4.683142
214.661778	7545.305401	14.361139	-0.046535	4.680738
214.573635	7537.281168	14.366144	-0.046514	4.678325
214.423720	7529.292958	14.371149	-0.046482	4.675920
214.524662	7521.205436	14.376154	-0.046496	4.673484
214.458554	7513.150342	14.381159	-0.046479	4.671057
214.225432	7505.200199	14.386163	-0.046432	4.668661
214.416067	7497.175288	14.391168	-0.046463	4.666240
214.595109	7489.251649	14.396173	-0.046492	4.663849
214.465588	7481.267787	14.401178	-0.046463	4.661438
214.135226	7473.232633	14.406183	-0.046397	4.659011
214.515350	7465.313673	14.411187	-0.046464	4.656617
214.117842	7457.218632	14.416192	-0.046385	4.654170
214.229452	7449.249203	14.421197	-0.046401	4.651758
214.146465	7441.174035	14.426202	-0.046382	4.649314
214.096434	7433.218652	14.431207	-0.046368	4.646904
214.308053	7425.186692	14.436211	-0.046403	4.644470
214.184980	7417.269295	14.441216	-0.046375	4.642069
214.234348	7409.201042	14.446221	-0.046380	4.639622
213.920214	7401.245364	14.451226	-0.046317	4.637207
213.920951	7393.186562	14.456231	-0.046313	4.634760
213.957282	7385.197818	14.461235	-0.046315	4.632332
213.867301	7377.107345	14.466240	-0.046294	4.629873
213.697146	7369.205833	14.471245	-0.046258	4.627470
213.844404	7361.171346	14.476250	-0.046281	4.625024
213.907730	7353.261958	14.481255	-0.046288	4.622616
213.559603	7345.167958	14.486259	-0.046219	4.620150
213.683360	7337.186079	14.491264	-0.046238	4.617717
213.747952	7329.191985	14.496269	-0.046245	4.615279
213.678393	7321.149941	14.501274	-0.046228	4.612826
213.382436	7313.113298	14.506279	-0.046168	4.610372
213.472223	7305.203485	14.511283	-0.046181	4.607956
213.629668	7297.140473	14.516288	-0.046206	4.605492
213.626463	7289.190058	14.521293	-0.046201	4.603061
213.262202	7281.176901	14.526298	-0.046128	4.600609
213.218366	7273.158586	14.531303	-0.046116	4.598154
213.213614	7265.193435	14.536307	-0.046110	4.595715
213.196494	7257.109301	14.541312	-0.046103	4.593237
213.315946	7249.107675	14.546317	-0.046121	4.590784
213.286551	7241.124833	14.551322	-0.046111	4.588335
213.311848	7233.107508	14.556327	-0.046111	4.585875
213.364359	7225.204182	14.561331	-0.046116	4.583447
213.245718	7217.158184	14.566336	-0.046090	4.580975
213.166429	7209.186524	14.571341	-0.046071	4.578524
213.021497	7201.114852	14.576346	-0.046039	4.576041
212.990245	7193.101012	14.581351	-0.046029	4.573575
212.840319	7185.093943	14.586355	-0.045997	4.571109
212.528105	7177.090827	14.591360	-0.045934	4.568643
212.717823	7169.140891	14.596365	-0.045965	4.566193
212.599058	7161.152866	14.601370	-0.045938	4.563729
212.485746	7153.133785	14.606375	-0.045913	4.561254
212.385751	7145.142300	14.611379	-0.045890	4.558786
212.679022	7137.104905	14.616384	-0.045940	4.556304
212.757067	7129.144495	14.621389	-0.045950	4.553843
212.596153	7121.102751	14.626394	-0.045916	4.551356
212.698031	7113.077238	14.631399	-0.045930	4.548873
212.539146	7105.121980	14.636403	-0.045896	4.546410
212.351980	7097.095692	14.641408	-0.045857	4.543923
212.483023	7089.150606	14.646413	-0.045877	4.541461
212.379052	7081.134682	14.651418	-0.045853	4.538975
212.183738	7073.176060	14.656423	-0.045812	4.536505
212.194735	7065.135104	14.661427	-0.045810	4.534008
212.014553	7057.096804	14.666432	-0.045772	4.531511
212.014889	7049.077875	14.671437	-0.045768	4.529019
212.020295	7041.092437	14.676442	-0.045764	4.526536
212.070622	7033.071948	14.681447	-0.045769	4.524040
212.103535	7025.154249	14.686451	-0.045771	4.521575
211.900693	7017.093317	14.691456	-0.045729	4.519064
211.844177	7009.172031	14.696461	-0.045714	4.516595
211.717640	7001.106520	14.701466	-0.045686	4.514080
211.719341	6993.004517	14.706471	-0.045682	4.511552
211.879948	6985.055720	14.711475	-0.045707	4.509071
211.708043	6977.033105	14.716480	-0.045671	4.506564
211.714373	6969.030469	14.721485	-0.045667	4.504063
211.452935	6961.101514	14.726490	-0.045614	4.501583
211.575925	6953.061850	14.731495	-0.045633	4.499068
211.352006	6945.124546	14.736499	-0.045587	4.496583
211.304313	6937.032632	14.741504	-0.045573	4.494048
211.342106	6929.038102	14.746509	-0.045576	4.491543
211.202938	6921.025867	14.751514	-0.045546	4.489030
211.216393	6913.091264	14.756519	-0.045544	4.486540
211.256092	6905.053426	14.761523	-0.045547	4.484017
211.321171	6897.077473	14.766528	-0.045554	4.481512
211.138505	6889.052960	14.771533	-0.045516	4.478989
211.097579	6881.086113	14.776538	-0.045504	4.476484
211.176239	6873.032172	14.781543	-0.045514	4.473950
211.238661	6865.044416	14.786547	-0.045521	4.471436
210.965200	6857.002517	14.791552	-0.045466	4.468902
210.939392	6849.042654	14.796557	-0.045457	4.466393
211.197422	6841.006757	14.801562	-0.045500	4.463859
211.215995	6833.054343	14.806567	-0.045499	4.461350
211.079177	6825.066760	14.811571	-0.045470	4.458828
211.035399	6817.024320	14.816576	-0.045457	4.456287
211.110191	6809.050183	14.821581	-0.045466	4.453767
210.845661	6800.994043	14.826586	-0.045413	4.451218
210.826213	6792.998654	14.831591	-0.045405	4.448688
210.736126	6785.005794	14.836595	-0.045384	4.446157
210.695508	6777.010959	14.841600	-0.045372	4.443625
210.584584	6769.035437	14.846605	-0.045346	4.441096
210.472983	6761.029089	14.851610	-0.045321	4.438556
210.407907	6753.038532	14.856615	-0.045305	4.436020
210.446315	6745.002960	14.861619	-0.045307	4.433469
210.234002	6736.938242	14.866624	-0.045263	4.430906
210.275134	6728.977716	14.871629	-0.045267	4.428375
210.254638	6720.959831	14.876634	-0.045258	4.425825
210.285459	6712.981126	14.881639	-0.045260	4.423286
210.433768	6704.990533	14.886643	-0.045283	4.420742
210.194702	6696.972171	14.891648	-0.045234	4.418186
210.119964	6688.995181	14.896653	-0.045216	4.415643
210.061398	6680.978542	14.901658	-0.045200	4.413085
210.049388	6672.946289	14.906663	-0.045194	4.410521
210.035282	6665.011592	14.911667	-0.045187	4.407987
209.867054	6656.941362	14.916672	-0.045151	4.405407
210.002604	6648.973457	14.921677	-0.045172	4.402861
209.943233	6640.954807	14.926682	-0.045156	4.400295
209.826909	6633.040293	14.931687	-0.045130	4.397761
209.749985	6624.999151	14.936691	-0.045111	4.395185
209.788412	6616.965654	14.941696	-0.045114	4.392610
209.691034	6608.945050	14.946701	-0.045092	4.390038
209.616212	6600.984242	14.951706	-0.045073	4.387483
209.690831	6592.939911	14.956711	-0.045083	4.384901
209.838706	6585.013629	14.961715	-0.045106	4.382356
209.591998	6576.955334	14.966720	-0.045055	4.379764
209.685573	6569.018931	14.971725	-0.045068	4.377212
209.523167	6560.991963	14.976730	-0.045034	4.374628
209.562306	6553.001907	14.981735	-0.045037	4.372055
209.708662	6544.933149	14.986739	-0.045059	4.369457
209.627781	6536.989649	14.991744	-0.045040	4.366895
209.375668	6529.008670	14.996749	-0.044989	4.364319
209.625929	6521.044010	15.001754	-0.045031	4.361750
209.466681	6512.990522	15.006759	-0.044997	4.359148
209.287623	6505.050479	15.011763	-0.044959	4.356582
209.223016	6496.963284	15.016768	-0.044942	4.353966
209.364789	6488.864264	15.021773	-0.044964	4.351347
209.167381	6480.889799	15.026778	-0.044923	4.348764
209.017442	6472.908579	15.031783	-0.044891	4.346178
208.951191	6464.916952	15.036787	-0.044874	4.343587
208.910176	6456.968091	15.041792	-0.044862	4.341009
208.918579	6449.017155	15.046797	-0.044859	4.338429
209.085362	6440.995473	15.051802	-0.044886	4.335826
208.933485	6432.901851	15.056807	-0.044853	4.333195
208.837297	6424.945447	15.061811	-0.044831	4.330608
208.710987	6416.927340	15.066816	-0.044803	4.327999
208.814382	6408.909992	15.071821	-0.044818	4.325390
208.651005	6400.965701	15.076826	-0.044783	4.322801
208.537897	6392.933164	15.081831	-0.044757	4.320183
208.649048	6384.945433	15.086835	-0.044774	4.317579
208.623371	6376.940750	15.091840	-0.044764	4.314967
208.551793	6368.951552	15.096845	-0.044747	4.312359
208.501323	6360.904629	15.101850	-0.044733	4.309730
208.657260	6352.913168	15.106855	-0.044757	4.307119
208.462078	6344.909058	15.111859	-0.044717	4.304499
208.100120	6336.941550	15.116864	-0.044645	4.301889
208.253281	6328.957082	15.121869	-0.044669	4.299276
208.350918	6320.908277	15.126874	-0.044683	4.296639
208.262595	6312.912722	15.131879	-0.044662	4.294017
208.148088	6304.913225	15.136883	-0.044636	4.291392
208.202585	6296.884048	15.141888	-0.044642	4.288756
208.397295	6288.907583	15.146893	-0.044674	4.286138
208.260984	6280.917696	15.151898	-0.044644	4.283511
208.248423	6272.930570	15.156903	-0.044637	4.280884
208.135706	6264.966101	15.161907	-0.044612	4.278262
208.045611	6256.960486	15.166912	-0.044590	4.275625
207.992401	6248.918160	15.171917	-0.044576	4.272975
207.797738	6240.870362	15.176922	-0.044535	4.270320
207.634131	6232.857108	15.181927	-0.044500	4.267675
207.828831	6224.861100	15.186931	-0.044532	4.265037
207.726565	6216.919505	15.191936	-0.044509	4.262413
207.447745	6208.889410	15.196941	-0.044452	4.259757
207.393597	6200.980068	15.201946	-0.044438	4.257140
207.635058	6192.894927	15.206951	-0.044479	4.254467
207.551875	6184.905732	15.211955	-0.044459	4.251821
207.473185	6176.845130	15.216960	-0.044439	4.249149
207.426813	6168.914870	15.221965	-0.044426	4.246520
207.311236	6160.899303	15.226970	-0.044401	4.243859
207.205275	6152.920508	15.231975	-0.044376	4.241210
207.358667	6144.929945	15.236979	-0.044401	4.238557
207.197994	6136.916738	15.241984	-0.044366	4.235892
207.119840	6128.920332	15.246989	-0.044347	4.233232
207.114474	6120.898736	15.251994	-0.044342	4.230562
207.055538	6112.920333	15.256999	-0.044326	4.227905
207.169875	6104.935305	15.262003	-0.044343	4.225245
207.021667	6096.916265	15.267008	-0.044311	4.222570
207.205319	6088.940154	15.272013	-0.044341	4.219911
206.982186	6080.957878	15.277018	-0.044295	4.217243
206.726827	6072.931275	15.282023	-0.044243	4.214559
206.922580	6064.918547	15.287027	-0.044275	4.211883
206.689970	6056.889462	15.292032	-0.044227	4.209195
206.763474	6048.954059	15.297037	-0.044237	4.206540
206.746161	6040.902529	15.302042	-0.044229	4.203843
206.646881	6032.938829	15.307047	-0.044206	4.201173
206.709764	6024.931395	15.312051	-0.044213	4.198488
206.482706	6016.925220	15.317056	-0.044167	4.195799
206.433611	6008.897231	15.322061	-0.044153	4.193103
206.545258	6000.805189	15.327066	-0.044169	4.190385
206.370199	5992.875193	15.332071	-0.044132	4.187717
206.378451	5984.885012	15.337075	-0.044129	4.185029
206.418624	5976.891509	15.342080	-0.044132	4.182339
206.224126	5968.901577	15.347085	-0.044092	4.179645
206.119078	5960.931519	15.352090	-0.044068	4.176957
206.067516	5952.897319	15.357095	-0.044054	4.174247
206.166523	5944.891076	15.362099	-0.044068	4.171546
206.089754	5936.872787	15.367104	-0.044049	4.168837
206.156191	5928.913087	15.372109	-0.044057	4.166147
206.025828	5920.915358	15.377114	-0.044028	4.163441
205.704937	5912.898964	15.382119	-0.043964	4.160725
205.947747	5904.952441	15.387123	-0.044005	4.158037
205.927363	5896.880058	15.392128	-0.043997	4.155301
205.972091	5888.865049	15.397133	-0.044001	4.152584
205.920539	5880.835642	15.402138	-0.043987	4.149859
206.096837	5872.865118	15.407143	-0.044015	4.147155
205.975785	5864.871649	15.412147	-0.043988	4.144438
205.659966	5856.903250	15.417152	-0.043925	4.141726
205.657911	5848.916155	15.422157	-0.043920	4.139009
205.763281	5840.895614	15.427162	-0.043935	4.136280
205.615174	5832.877570	15.432167	-0.043903	4.133547
205.441121	5824.854850	15.437171	-0.043866	4.130810
205.500541	5816.863774	15.442176	-0.043873	4.128085
205.393441	5808.881322	15.447181	-0.043849	4.125359
205.383918	5800.909734	15.452186	-0.043842	4.122636
205.315900	5792.861579	15.457191	-0.043825	4.119885
205.383494	5784.975305	15.462195	-0.043834	4.117189
205.285076	5776.855073	15.467200	-0.043811	4.114409
205.439552	5768.846595	15.472205	-0.043835	4.111668
205.374366	5760.842605	15.477210	-0.043819	4.108925
205.099190	5752.856534	15.482215	-0.043763	4.106183
205.241432	5744.855407	15.487219	-0.043785	4.103439
205.082018	5736.879352	15.492224	-0.043751	4.100698
205.017877	5728.935902	15.497229	-0.043735	4.097968
204.765967	5720.897053	15.502234	-0.043683	4.095201
204.861976	5712.886457	15.507239	-0.043697	4.092446
205.023230	5704.865066	15.512243	-0.043722	4.089686
204.948882	5696.896357	15.517248	-0.043704	4.086940
204.890025	5688.888070	15.522253	-0.043689	4.084178
204.896486	5680.983045	15.527258	-0.043685	4.081451
204.798790	5672.918418	15.532263	-0.043663	4.078666
204.888213	5664.985534	15.537267	-0.043675	4.075926
204.809266	5656.908564	15.542272	-0.043656	4.073133
204.831187	5648.875484	15.547277	-0.043655	4.070354
204.641475	5640.917816	15.552282	-0.043616	4.067597
204.466268	5632.902870	15.557287	-0.043579	4.064818
204.690007	5624.963501	15.562291	-0.043616	4.062069
204.361875	5616.919972	15.567296	-0.043550	4.059274
204.276271	5608.986238	15.572301	-0.043530	4.056519
204.345260	5600.940973	15.577306	-0.043538	4.053726
204.110349	5592.910378	15.582311	-0.043490	4.050931
204.143016	5584.943247	15.587315	-0.043492	4.048160
204.113742	5576.888246	15.592320	-0.043482	4.045356
204.156669	5568.961217	15.597325	-0.043486	4.042595
203.966822	5560.937606	15.602330	-0.043446	4.039796
203.895031	5552.971843	15.607335	-0.043428	4.037016
204.186413	5544.912804	15.612339	-0.043478	4.034208
204.046823	5536.811790	15.617344	-0.043447	4.031376
204.040289	5528.839323	15.622349	-0.043442	4.028590
204.124980	5520.873751	15.627354	-0.043453	4.025805
203.727812	5512.921415	15.632359	-0.043375	4.023015
203.789277	5504.922490	15.637363	-0.043382	4.020214
203.593145	5496.912912	15.642368	-0.043341	4.017404
203.794537	5488.898483	15.647373	-0.043374	4.014596
203.662490	5480.902683	15.652378	-0.043345	4.011788
203.513674	5472.899966	15.657383	-0.043313	4.008974
203.593267	5464.916627	15.662387	-0.043323	4.006169
203.411111	5456.910757	15.667392	-0.043285	4.003351
203.430386	5448.907669	15.672397	-0.043284	4.000534
203.520962	5440.952150	15.677402	-0.043296	3.997733
203.432822	5432.912079	15.682407	-0.043276	3.994898
203.519550	5424.918379	15.687411	-0.043287	3.992080
203.281549	5416.879862	15.692416	-0.043239	3.989238
203.267629	5408.914534	15.697421	-0.043232	3.986424
203.112416	5400.905800	15.702426	-0.043198	3.983591
202.834656	5392.909446	15.707431	-0.043142	3.980758
202.972976	5384.943454	15.712435	-0.043163	3.977940
202.937585	5376.937502	15.717440	-0.043152	3.975103
202.762460	5368.943899	15.722445	-0.043115	3.972267
202.884814	5360.883886	15.727450	-0.043134	3.969409
202.871653	5352.933675	15.732455	-0.043127	3.966587
202.772914	5344.965124	15.737459	-0.043104	3.963754
202.831739	5336.956989	15.742464	-0.043111	3.960908
202.814556	5328.988086	15.747469	-0.043103	3.958073
202.754774	5320.982267	15.752474	-0.043087	3.955222
202.606743	5312.934868	15.757479	-0.043055	3.952352
202.686541	5304.907630	15.762483	-0.043066	3.949491
202.415817	5296.944489	15.767488	-0.043011	3.946645
202.492573	5288.948241	15.772493	-0.043021	3.943791
202.269176	5280.966486	15.777498	-0.042975	3.940935
202.436177	5272.957269	15.782503	-0.043002	3.938074
202.404915	5264.976771	15.787507	-0.042991	3.935218
202.419947	5256.920464	15.792512	-0.042990	3.932333
202.352706	5248.927322	15.797517	-0.042973	3.929467
202.179309	5241.008923	15.802522	-0.042936	3.926625
202.016844	5232.991435	15.807527	-0.042901	3.923744
202.029909	5225.003139	15.812531	-0.042899	3.920875
202.214265	5216.945963	15.817536	-0.042929	3.917983
202.166984	5209.021053	15.822541	-0.042916	3.915132
201.899865	5200.971050	15.827546	-0.042862	3.912229
201.868200	5192.955713	15.832551	-0.042852	3.909341
201.914797	5185.005461	15.837555	-0.042856	3.906476
201.710130	5177.009206	15.842560	-0.042813	3.903588
201.807609	5168.998012	15.847565	-0.042827	3.900697
201.989811	5161.002105	15.852570	-0.042856	3.897812
201.591121	5152.983017	15.857575	-0.042778	3.894905
201.753957	5144.966346	15.862579	-0.042804	3.892008
201.885847	5136.936534	15.867584	-0.042824	3.889102
201.591513	5128.997327	15.872589	-0.042765	3.886220
201.644808	5120.989664	15.877594	-0.042770	3.883317
201.762247	5112.949281	15.882599	-0.042788	3.880401
201.756860	5105.046089	15.887603	-0.042782	3.877531
201.635664	5096.981554	15.892608	-0.042755	3.874598
201.581977	5088.768527	15.897613	-0.042741	3.871609
201.607563	5080.818190	15.902618	-0.042741	3.868716
201.288198	5072.882312	15.907623	-0.042677	3.865819
201.359169	5064.937170	15.912627	-0.042686	3.862924
201.219975	5056.932508	15.917632	-0.042656	3.860000
201.372604	5049.010215	15.922637	-0.042680	3.857111
201.034785	5040.979976	15.927642	-0.042612	3.854170
201.388798	5032.953492	15.932647	-0.042674	3.851242
201.184087	5024.992202	15.937651	-0.042631	3.848325
201.022415	5016.950276	15.942656	-0.042597	3.845376
201.276758	5009.001973	15.947661	-0.042640	3.842469
201.205735	5001.003855	15.952666	-0.042622	3.839534
200.965818	4993.063927	15.957671	-0.042573	3.836614
201.091273	4985.061040	15.962675	-0.042592	3.833677
200.975117	4976.986283	15.967680	-0.042566	3.830706
201.072138	4969.008330	15.972685	-0.042579	3.827773
200.959462	4961.024716	15.977690	-0.042554	3.824831
200.912550	4953.039289	15.982695	-0.042541	3.821888
200.879871	4945.059219	15.987699	-0.042530	3.818944
200.646392	4937.091003	15.992704	-0.042482	3.815999
200.799724	4929.065218	15.997709	-0.042507	3.813038
200.643281	4921.048426	16.002714	-0.042473	3.810071
200.381478	4913.096404	16.007719	-0.042420	3.807124
200.450819	4905.062988	16.012723	-0.042428	3.804152
200.324393	4897.100391	16.017728	-0.042400	3.801199
200.287995	4889.097494	16.022733	-0.042389	3.798231
200.348296	4881.109451	16.027738	-0.042396	3.795268
200.378909	4873.040310	16.032743	-0.042397	3.792272
200.343586	4865.059551	16.037747	-0.042386	3.789305
200.209355	4857.059086	16.042752	-0.042357	3.786326
200.083617	4849.109742	16.047757	-0.042329	3.783365
200.176833	4841.066403	16.052762	-0.042342	3.780370
200.145152	4833.070412	16.057767	-0.042332	3.777388
199.891911	4825.089973	16.062771	-0.042280	3.774405
199.811706	4817.080388	16.067776	-0.042261	3.771412
199.891964	4809.064091	16.072781	-0.042271	3.768418
199.697474	4801.094276	16.077786	-0.042231	3.765433
199.599594	4793.097439	16.082791	-0.042208	3.762438
199.715148	4785.086405	16.087795	-0.042225	3.759439
199.768228	4777.133013	16.092800	-0.042230	3.756459
199.727915	4769.125984	16.097805	-0.042219	3.753453
199.753336	4761.050675	16.102810	-0.042219	3.750422
199.528970	4753.091264	16.107815	-0.042173	3.747425
199.521565	4745.090761	16.112819	-0.042167	3.744416
199.451866	4737.141221	16.117824	-0.042149	3.741422
199.569866	4729.105109	16.122829	-0.042167	3.738397
199.479018	4721.127514	16.127834	-0.042146	3.735387
199.387722	4713.128302	16.132839	-0.042124	3.732367
199.599858	4705.098197	16.137843	-0.042159	3.729339
199.414434	4697.127874	16.142848	-0.042120	3.726323
199.271712	4689.150643	16.147853	-0.042089	3.723302
199.074594	4681.190851	16.152858	-0.042048	3.720284
199.065124	4673.211568	16.157863	-0.042042	3.717260
199.011006	4665.196393	16.162867	-0.042028	3.714220
198.889414	4657.065530	16.167872	-0.042000	3.711131
198.988118	4649.078409	16.172877	-0.042014	3.708100
198.872533	4641.124832	16.177882	-0.041988	3.705074
198.990795	4633.141249	16.182887	-0.042006	3.702040
198.915188	4625.172730	16.187891	-0.041988	3.699004
198.712959	4617.191243	16.192896	-0.041946	3.695957
198.853926	4609.179968	16.197901	-0.041967	3.692906
198.849300	4601.179130	16.202906	-0.041962	3.689852
198.690522	4593.200828	16.207911	-0.041928	3.686800
198.588800	4585.223793	16.212915	-0.041905	3.683747
198.447003	4577.236509	16.217920	-0.041874	3.680688
198.736824	4569.241825	16.222925	-0.041923	3.677633
198.640217	4561.195636	16.227930	-0.041901	3.674547
198.513539	4553.177795	16.232935	-0.041873	3.671468
198.573462	4545.200521	16.237939	-0.041880	3.668407
198.327367	4537.206669	16.242944	-0.041829	3.665329
198.227370	4529.238163	16.247949	-0.041806	3.662262
198.358810	4521.216900	16.252954	-0.041826	3.659178
198.256588	4513.262795	16.257959	-0.041803	3.656111
198.180755	4505.254526	16.262963	-0.041784	3.653022
198.148054	4497.205641	16.267968	-0.041774	3.649915
198.119163	4489.265985	16.272973	-0.041764	3.646848
198.133418	4481.259818	16.277978	-0.041762	3.643754
198.122332	4473.255744	16.282983	-0.041756	3.640657
198.161332	4465.290487	16.287987	-0.041759	3.637574
198.135810	4457.263970	16.292992	-0.041750	3.634463
197.893579	4449.244133	16.297997	-0.041700	3.631346
197.737961	4441.246152	16.303002	-0.041667	3.628237
197.710647	4433.222830	16.308007	-0.041657	3.625119
197.758280	4425.291050	16.313011	-0.041662	3.622036
197.659185	4417.252046	16.318016	-0.041639	3.618905
197.737521	4409.290849	16.323021	-0.041649	3.615806
197.584848	4401.304760	16.328026	-0.041616	3.612688
197.430100	4393.275401	16.333031	-0.041583	3.609551
197.622163	4385.329110	16.338035	-0.041614	3.606453
197.483834	4377.309340	16.343040	-0.041584	3.603314
197.333679	4369.352507	16.348045	-0.041552	3.600197
197.250354	4361.358794	16.353050	-0.041532	3.597065
197.378972	4353.335347	16.358055	-0.041551	3.593924
197.499320	4345.332186	16.363059	-0.041569	3.590789
197.245769	4337.335171	16.368064	-0.041518	3.587642
197.251206	4329.355905	16.373069	-0.041514	3.584507
197.287975	4321.406735	16.378074	-0.041517	3.581382
197.052160	4313.387632	16.383079	-0.041468	3.578218
197.082116	4305.416512	16.388083	-0.041469	3.575079
197.035370	4297.383613	16.393088	-0.041456	3.571910
196.950222	4289.401803	16.398093	-0.041436	3.568758
196.977488	4281.398272	16.403098	-0.041437	3.565597
197.142911	4273.405835	16.408103	-0.041463	3.562442
197.114573	4265.405574	16.413107	-0.041453	3.559275
196.895559	4257.443932	16.418112	-0.041408	3.556115
196.834158	4249.354158	16.423117	-0.041392	3.552906
196.649854	4241.333585	16.428122	-0.041353	3.549719
196.597360	4233.356018	16.433127	-0.041339	3.546549
196.502597	4225.426462	16.438131	-0.041317	3.543394
196.644803	4217.398353	16.443136	-0.041339	3.540204
196.702389	4209.407305	16.448141	-0.041346	3.537024
196.568409	4201.417543	16.453146	-0.041316	3.533835
196.397583	4193.393262	16.458151	-0.041280	3.530629
196.307360	4185.446816	16.463155	-0.041259	3.527453
196.140720	4177.424380	16.468160	-0.041223	3.524242
196.132232	4169.471369	16.473165	-0.041217	3.521061
196.352463	4161.448816	16.478170	-0.041254	3.517855
196.207401	4153.473965	16.483175	-0.041222	3.514655
196.287936	4145.490651	16.488179	-0.041233	3.511455
196.210872	4137.452118	16.493184	-0.041214	3.508225
196.164763	4129.469108	16.498189	-0.041201	3.505016
196.096877	4121.525377	16.503194	-0.041184	3.501819
196.021397	4113.513567	16.508199	-0.041166	3.498591
196.085274	4105.544022	16.513203	-0.041173	3.495381
195.830681	4097.545519	16.518208	-0.041121	3.492147
196.072948	4089.507151	16.523213	-0.041162	3.488910
195.937991	4081.534309	16.528218	-0.041132	3.485684
195.669781	4073.586338	16.533223	-0.041078	3.482461
195.668799	4065.584699	16.538227	-0.041074	3.479221
195.720227	4057.594074	16.543232	-0.041079	3.475985
195.766282	4049.574367	16.548237	-0.041083	3.472734
195.454305	4041.556005	16.553242	-0.041020	3.469468
195.523142	4033.554177	16.558247	-0.041029	3.466219
195.676513	4025.584532	16.563251	-0.041053	3.462983
195.392650	4017.572944	16.568256	-0.040996	3.459712
195.272851	4009.640904	16.573261	-0.040969	3.456475
195.499824	4001.578309	16.578266	-0.041007	3.453194
195.368002	3993.578177	16.583271	-0.040978	3.449923
195.145111	3985.646502	16.588275	-0.040932	3.446675
195.046275	3977.630743	16.593280	-0.040909	3.443393
195.111629	3969.628400	16.598285	-0.040917	3.440118
194.962033	3961.691491	16.603290	-0.040884	3.436860
195.229495	3953.625477	16.608295	-0.040930	3.433560
195.223576	3945.649479	16.613299	-0.040924	3.430285
195.217746	3937.633268	16.618304	-0.040919	3.426990
194.988354	3929.665132	16.623309	-0.040872	3.423704
195.077580	3921.683825	16.628314	-0.040884	3.420421
194.847571	3913.712266	16.633319	-0.040837	3.417127
194.822408	3905.717946	16.638323	-0.040828	3.413828
194.693995	3897.694597	16.643328	-0.040799	3.410509
194.768245	3889.718132	16.648333	-0.040809	3.407214
194.681066	3881.747716	16.653338	-0.040788	3.403913
194.421162	3873.791963	16.658343	-0.040735	3.400609
194.506149	3865.801659	16.663347	-0.040747	3.397299
194.500437	3857.751527	16.668352	-0.040741	3.393958
194.517636	3849.675104	16.673357	-0.040740	3.390603
194.432270	3841.725616	16.678362	-0.040719	3.387295
194.429479	3833.709496	16.683367	-0.040715	3.383958
194.529709	3825.772697	16.688371	-0.040729	3.380654
194.335398	3817.804260	16.693376	-0.040688	3.377324
194.260973	3809.812654	16.698381	-0.040670	3.373985
194.097644	3801.802227	16.703386	-0.040635	3.370632
194.023784	3793.821299	16.708391	-0.040617	3.367291
194.082812	3785.852602	16.713395	-0.040624	3.363956
193.840775	3777.859548	16.718400	-0.040574	3.360597
193.890959	3769.865089	16.723405	-0.040579	3.357245
194.102029	3761.840208	16.728410	-0.040614	3.353882
193.855634	3753.804907	16.733415	-0.040563	3.350495
193.769401	3745.848509	16.738419	-0.040543	3.347143
193.701536	3737.883714	16.743424	-0.040526	3.343786
193.660436	3729.906868	16.748429	-0.040514	3.340420
193.599341	3721.931693	16.753434	-0.040498	3.337052
193.455392	3713.900948	16.758439	-0.040467	3.333653
193.482868	3705.904767	16.763443	-0.040468	3.330272
193.342214	3697.913024	16.768448	-0.040437	3.326883
193.488799	3689.921167	16.773453	-0.040460	3.323501
193.418304	3681.959450	16.778458	-0.040442	3.320121
193.479969	3673.978041	16.783463	-0.040449	3.316734
193.448564	3665.978502	16.788467	-0.040439	3.313331
193.215553	3657.951558	16.793472	-0.040391	3.309907
193.148782	3649.958539	16.798477	-0.040374	3.306499
193.108786	3641.988238	16.803482	-0.040363	3.303098
193.159137	3633.991054	16.808487	-0.040368	3.299686
193.097885	3626.052996	16.813491	-0.040352	3.296292
193.059332	3618.037229	16.818496	-0.040340	3.292861
193.003472	3610.018275	16.823501	-0.040325	3.289425
193.096103	3602.037301	16.828506	-0.040338	3.286008
192.971301	3594.067488	16.833511	-0.040310	3.282583
192.804577	3586.098951	16.838515	-0.040275	3.279153
192.752359	3578.102331	16.843520	-0.040261	3.275713
192.808013	3570.079699	16.848525	-0.040267	3.272261
192.952196	3562.070480	16.853530	-0.040289	3.268815
192.741250	3554.071655	16.858535	-0.040246	3.265357
192.867787	3546.126424	16.863539	-0.040265	3.261931
192.833841	3538.111797	16.868544	-0.040254	3.258464
192.436670	3530.159968	16.873549	-0.040176	3.255007
192.510187	3522.168439	16.878554	-0.040185	3.251548
192.475334	3514.150764	16.883559	-0.040174	3.248070
192.352809	3506.181418	16.888563	-0.040147	3.244605
192.017101	3498.221715	16.893568	-0.040080	3.241132
192.270219	3490.189551	16.898573	-0.040122	3.237648
192.266902	3482.211241	16.903578	-0.040117	3.234172
191.985308	3474.150075	16.908583	-0.040061	3.230646
191.996426	3466.179177	16.913587	-0.040058	3.227167
191.894431	3458.190320	16.918592	-0.040035	3.223672
191.889892	3450.216736	16.923597	-0.040030	3.220184
191.854437	3442.258973	16.928602	-0.040019	3.216698
191.838431	3434.238279	16.933607	-0.040011	3.213181
191.990878	3426.233238	16.938611	-0.040035	3.209674
191.921420	3418.267075	16.943616	-0.040018	3.206171
191.949780	3410.295426	16.948621	-0.040019	3.202666
191.858154	3402.330412	16.953626	-0.039997	3.199155
191.500752	3394.378933	16.958631	-0.039926	3.195635
191.801686	3386.322762	16.963635	-0.039978	3.192092
191.860941	3378.304110	16.968640	-0.039984	3.188552
191.749814	3370.349435	16.973645	-0.039959	3.185029
191.575713	3362.415290	16.978650	-0.039922	3.181509
191.509829	3354.386002	16.983655	-0.039906	3.177947
191.609725	3346.402527	16.988659	-0.039920	3.174409
191.297139	3338.408688	16.993664	-0.039857	3.170844
191.364058	3330.416087	16.998669	-0.039865	3.167292
191.503236	3322.429627	17.003674	-0.039887	3.163742
191.201542	3314.467537	17.008679	-0.039826	3.160180
191.187791	3306.498469	17.013683	-0.039819	3.156623
191.135277	3298.452079	17.018688	-0.039805	3.153026
190.875547	3290.461629	17.023693	-0.039752	3.149440
190.979448	3282.486655	17.028698	-0.039767	3.145874
190.996240	3274.466571	17.033703	-0.039766	3.142279
190.931540	3266.540823	17.038707	-0.039750	3.138719
190.829530	3258.548610	17.043712	-0.039726	3.135124
190.907385	3250.552745	17.048717	-0.039736	3.131530
190.962106	3242.541978	17.053722	-0.039742	3.127925
190.613070	3234.572758	17.058727	-0.039673	3.124316
190.760453	3226.614855	17.063731	-0.039696	3.120730
190.711709	3218.628894	17.068736	-0.039682	3.117119
190.643802	3210.623779	17.073741	-0.039665	3.113494
190.741215	3202.601203	17.078746	-0.039679	3.109865
190.561039	3194.636319	17.083751	-0.039641	3.106244
190.661157	3186.656876	17.088755	-0.039655	3.102626
190.525359	3178.662307	17.093760	-0.039625	3.098986
190.305390	3170.719252	17.098765	-0.039580	3.095361
190.338515	3162.703296	17.103770	-0.039582	3.091710
190.396336	3154.705244	17.108775	-0.039588	3.088064
190.558913	3146.717634	17.113779	-0.039614	3.084423
190.419960	3138.763766	17.118784	-0.039584	3.080780
190.348509	3130.790720	17.123789	-0.039566	3.077127
190.167899	3122.785180	17.128794	-0.039528	3.073449
190.188105	3114.680479	17.133799	-0.039527	3.069731
190.159787	3106.764377	17.138803	-0.039517	3.066092
189.866193	3098.815623	17.143808	-0.039458	3.062422
189.929832	3090.824378	17.148813	-0.039466	3.058745
190.042787	3082.822766	17.153818	-0.039482	3.055060
189.772840	3074.839702	17.158823	-0.039428	3.051362
189.634115	3066.880612	17.163827	-0.039398	3.047677
189.691608	3058.856366	17.168832	-0.039404	3.043966
189.668892	3050.911441	17.173837	-0.039395	3.040283
189.565979	3042.967647	17.178842	-0.039372	3.036593
189.405082	3034.936138	17.183847	-0.039337	3.032855
189.673401	3026.916951	17.188851	-0.039383	3.029138
189.605399	3018.931778	17.193856	-0.039366	3.025417
189.603390	3010.976346	17.198861	-0.039361	3.021708
189.476528	3003.003631	17.203866	-0.039333	3.017980
189.311211	2995.014820	17.208871	-0.039298	3.014239
189.395643	2987.018474	17.213875	-0.039309	3.010501
189.448717	2979.029318	17.218880	-0.039314	3.006760
189.300014	2971.069331	17.223885	-0.039282	3.003019
189.139487	2963.119260	17.228890	-0.039248	2.999277
188.848059	2955.150570	17.233895	-0.039189	2.995515
189.107737	2947.107844	17.238899	-0.039233	2.991741
188.710620	2939.125618	17.243904	-0.039155	2.987958
188.649226	2931.138514	17.248909	-0.039139	2.984184
188.712374	2923.175347	17.253914	-0.039146	2.980423
188.660486	2915.181730	17.258919	-0.039132	2.976638
188.596460	2907.198289	17.263923	-0.039116	2.972851
188.517397	2899.191812	17.268928	-0.039097	2.969048
188.520730	2891.222258	17.273933	-0.039093	2.965262
188.480871	2883.257682	17.278938	-0.039081	2.961471
188.375935	2875.285439	17.283943	-0.039057	2.957669
188.402121	2867.306093	17.288947	-0.039058	2.953865
188.355157	2859.275662	17.293952	-0.039045	2.950027
188.129026	2851.311628	17.298957	-0.038998	2.946208
188.205848	2843.333671	17.303962	-0.039008	2.942392
188.194688	2835.350846	17.308967	-0.039001	2.938564
188.201784	2827.406337	17.313971	-0.038998	2.934751
187.849964	2819.386643	17.318976	-0.038928	2.930878
188.090435	2811.367521	17.323981	-0.038969	2.927031
187.816391	2803.454572	17.328986	-0.038913	2.923203
187.939799	2795.430360	17.333991	-0.038932	2.919338
188.138386	2787.484000	17.338995	-0.038964	2.915508
187.805466	2779.438762	17.344000	-0.038898	2.911598
187.702278	2771.431364	17.349005	-0.038874	2.907713
187.811342	2763.463391	17.354010	-0.038890	2.903853
187.601071	2755.518769	17.359015	-0.038847	2.899983
187.691398	2747.559921	17.364019	-0.038859	2.896116
187.585049	2739.557247	17.369024	-0.038835	2.892212
187.779050	2731.551251	17.374029	-0.038867	2.888318
187.723058	2723.592713	17.379034	-0.038852	2.884428
187.470814	2715.648959	17.384039	-0.038800	2.880529
187.509014	2707.680470	17.389043	-0.038803	2.876629
187.604898	2699.645699	17.394048	-0.038817	2.872694
187.245103	2691.704079	17.399053	-0.038745	2.868774
187.325444	2683.701256	17.404058	-0.038756	2.864843
187.335702	2675.729290	17.409063	-0.038753	2.860918
187.269693	2667.780644	17.414067	-0.038737	2.856995
187.136192	2659.788648	17.419072	-0.038707	2.853041
187.406231	2651.764712	17.424077	-0.038753	2.849089
187.376815	2643.788187	17.429082	-0.038743	2.845138
186.936237	2635.880085	17.434087	-0.038657	2.841192
187.033580	2627.907641	17.439091	-0.038671	2.837239
186.960454	2619.889110	17.444096	-0.038652	2.833248
186.762682	2611.891739	17.449101	-0.038611	2.829254
187.011172	2603.894220	17.454106	-0.038653	2.825281
186.924054	2595.928709	17.459111	-0.038632	2.821298
186.870741	2587.968122	17.464115	-0.038618	2.817315
186.678038	2579.981864	17.469120	-0.038578	2.813304
186.508271	2571.999483	17.474125	-0.038542	2.809292
186.751136	2564.014626	17.479130	-0.038583	2.805296
186.262617	2556.091254	17.484135	-0.038487	2.801283
186.547804	2548.095684	17.489139	-0.038536	2.797273
186.399170	2540.101011	17.494144	-0.038504	2.793232
186.373952	2532.092562	17.499149	-0.038495	2.789185
186.381220	2524.128976	17.504154	-0.038492	2.785158
186.146264	2516.178595	17.509159	-0.038444	2.781116
186.204235	2508.212534	17.514163	-0.038450	2.777079
186.038779	2500.241112	17.519168	-0.038415	2.773019
186.060877	2492.224581	17.524173	-0.038414	2.768942
185.980122	2484.267393	17.529178	-0.038395	2.764883
185.764488	2476.320633	17.534183	-0.038350	2.760815
185.929998	2468.340930	17.539187	-0.038377	2.756747
186.061044	2460.275174	17.544192	-0.038397	2.752627
185.867982	2452.294304	17.549197	-0.038356	2.748524
185.644265	2444.358850	17.554202	-0.038310	2.744437
185.738699	2436.349178	17.559207	-0.038323	2.740325
185.803461	2428.404061	17.564211	-0.038331	2.736239
185.550116	2420.430467	17.569216	-0.038280	2.732112
185.654661	2412.428953	17.574221	-0.038295	2.727986
185.689528	2404.476723	17.579226	-0.038297	2.723875
185.254869	2396.576784	17.584231	-0.038211	2.719756
185.386192	2388.581793	17.589235	-0.038231	2.715617
185.371427	2380.573155	17.594240	-0.038224	2.711455
185.224611	2372.613016	17.599245	-0.038193	2.707304
185.334832	2364.628941	17.604250	-0.038209	2.703149
185.237087	2356.645608	17.609255	-0.038186	2.698976
185.336271	2348.686176	17.614259	-0.038200	2.694822
185.173245	2340.701458	17.619264	-0.038165	2.690631
184.977479	2332.744524	17.624269	-0.038124	2.686445
185.182964	2324.765824	17.629274	-0.038158	2.682268
184.927830	2316.809567	17.634279	-0.038106	2.678066
184.910285	2308.861978	17.639283	-0.038099	2.673878
185.009662	2300.802101	17.644288	-0.038113	2.669631
184.652705	2292.873084	17.649293	-0.038042	2.665417
184.658596	2284.913754	17.654298	-0.038039	2.661204
184.394889	2276.951695	17.659303	-0.037985	2.656965
184.628923	2268.945146	17.664307	-0.038024	2.652728
184.334079	2260.986996	17.669312	-0.037965	2.648476
184.293414	2253.013247	17.674317	-0.037953	2.644225
184.306528	2245.063559	17.679322	-0.037951	2.639984
184.276610	2237.095455	17.684327	-0.037941	2.635723
184.279070	2229.098384	17.689331	-0.037937	2.631442
184.265615	2221.112214	17.694336	-0.037930	2.627158
184.263623	2213.144621	17.699341	-0.037925	2.622879
184.230192	2205.184934	17.704346	-0.037915	2.618594
184.108205	2197.219171	17.709351	-0.037888	2.614293
184.160276	2189.231959	17.714355	-0.037893	2.609986
184.006936	2181.271911	17.719360	-0.037860	2.605672
183.858865	2173.333401	17.724365	-0.037828	2.601363
183.989651	2165.371890	17.729370	-0.037848	2.597053
183.912354	2157.272424	17.734375	-0.037829	2.592646
183.746665	2149.240238	17.739379	-0.037794	2.588263
183.809779	2141.286889	17.744384	-0.037801	2.583931
183.589651	2133.374117	17.749389	-0.037756	2.579595
183.322039	2125.479889	17.754394	-0.037702	2.575258
183.376314	2117.461806	17.759399	-0.037707	2.570868
183.577335	2109.493704	17.764403	-0.037740	2.566508
183.457269	2101.555467	17.769408	-0.037714	2.562135
183.302929	2093.619046	17.774413	-0.037680	2.557753
183.355482	2085.643806	17.779418	-0.037686	2.553356
183.371719	2077.617740	17.784423	-0.037684	2.548922
183.382114	2069.673970	17.789427	-0.037682	2.544524
183.331362	2061.730050	17.794432	-0.037668	2.540115
183.310311	2053.766125	17.799437	-0.037660	2.535689
183.152264	2045.803618	17.804442	-0.037626	2.531246
183.108095	2037.820477	17.809447	-0.037613	2.526792
183.090798	2029.884010	17.814451	-0.037606	2.522358
182.959610	2021.927328	17.819456	-0.037577	2.517897
183.064228	2013.942289	17.824461	-0.037592	2.513429
183.047214	2005.940085	17.829466	-0.037584	2.508934
182.728491	1997.993032	17.834471	-0.037521	2.504441
182.674855	1990.064694	17.839475	-0.037506	2.499969
182.557943	1982.101282	17.844480	-0.037480	2.495465
182.753483	1974.089540	17.849485	-0.037512	2.490949
182.558232	1966.142573	17.854490	-0.037471	2.486432
182.413496	1958.201953	17.859495	-0.037440	2.481914
182.583683	1950.233290	17.864499	-0.037467	2.477395
182.586041	1942.257923	17.869504	-0.037463	2.472852
182.329232	1934.293556	17.874509	-0.037411	2.468287
182.553252	1926.311294	17.879514	-0.037448	2.463740
182.314323	1918.373393	17.884519	-0.037400	2.459174
182.193436	1910.437631	17.889523	-0.037373	2.454611
182.058156	1902.482509	17.894528	-0.037343	2.450027
182.220661	1894.478068	17.899533	-0.037369	2.445428
182.176627	1886.553564	17.904538	-0.037356	2.440851
182.033356	1878.598491	17.909543	-0.037325	2.436240
182.158077	1870.558338	17.914547	-0.037344	2.431591
182.125802	1862.567642	17.919552	-0.037334	2.426951
181.960980	1854.632030	17.924557	-0.037298	2.422323
181.891565	1846.713489	17.929562	-0.037281	2.417703
181.838991	1838.736294	17.934567	-0.037267	2.413042
181.867711	1830.774131	17.939571	-0.037268	2.408387
181.746806	1822.813450	17.944576	-0.037241	2.403712
181.696749	1814.888093	17.949581	-0.037227	2.399055
181.507477	1806.969692	17.954586	-0.037188	2.394381
181.343097	1798.974920	17.959591	-0.037153	2.389655
181.533814	1790.986550	17.964595	-0.037184	2.384952
181.375003	1783.055379	17.969600	-0.037150	2.380245
181.151415	1775.127908	17.974605	-0.037104	2.375526
181.219853	1767.150302	17.979610	-0.037112	2.370791
181.150848	1759.182197	17.984615	-0.037095	2.366042
181.265190	1751.225535	17.989619	-0.037112	2.361304
181.226510	1743.268370	17.994624	-0.037100	2.356544
181.019264	1735.312856	17.999629	-0.037057	2.351762
180.911545	1727.357575	18.004634	-0.037033	2.346978
180.719973	1719.407384	18.009639	-0.036993	2.342181
180.808585	1711.444354	18.014643	-0.037005	2.337389
181.016053	1703.453022	18.019648	-0.037039	2.332580
180.707706	1695.527888	18.024653	-0.036977	2.327759
180.679215	1687.586354	18.029658	-0.036967	2.322940
180.565443	1679.638563	18.034663	-0.036942	2.318101
180.527158	1671.703255	18.039667	-0.036930	2.313265
180.533763	1663.712227	18.044672	-0.036927	2.308390
180.487033	1655.756850	18.049677	-0.036914	2.303521
180.362056	1647.837194	18.054682	-0.036886	2.298657
180.187444	1639.891686	18.059687	-0.036850	2.293762
180.142792	1631.934200	18.064691	-0.036837	2.288861
180.414177	1623.944892	18.069696	-0.036883	2.283957
180.090446	1616.043862	18.074701	-0.036818	2.279045
180.113564	1608.080146	18.079706	-0.036818	2.274114
180.196843	1600.024125	18.084711	-0.036829	2.269120
180.216453	1592.089572	18.089715	-0.036829	2.264186
180.094149	1584.161983	18.094720	-0.036801	2.259232
179.862515	1576.250829	18.099725	-0.036754	2.254268
179.926874	1568.270725	18.104730	-0.036761	2.249276
179.805697	1560.328180	18.109735	-0.036735	2.244280
179.824736	1552.399675	18.114739	-0.036734	2.239295
179.891457	1544.441080	18.119744	-0.036742	2.234283
179.722452	1536.495526	18.124749	-0.036706	2.229247
179.745157	1528.552722	18.129754	-0.036706	2.224219
179.573935	1520.626575	18.134759	-0.036669	2.219173
179.580874	1512.682244	18.139763	-0.036666	2.214119
179.210184	1504.754656	18.144768	-0.036593	2.209031
179.246228	1496.795569	18.149773	-0.036595	2.203947
179.090266	1488.880927	18.154778	-0.036562	2.198862
179.124961	1480.910634	18.159783	-0.036564	2.193748
179.224596	1472.919413	18.164787	-0.036578	2.188614
179.106210	1464.972917	18.169792	-0.036552	2.183476
178.979113	1457.052451	18.174797	-0.036524	2.178343
178.905050	1449.122023	18.179802	-0.036505	2.173196
178.981036	1441.150914	18.184807	-0.036515	2.168024
179.034558	1433.206021	18.189811	-0.036521	2.162855
178.917296	1425.304906	18.194816	-0.036494	2.157686
178.823610	1417.359623	18.199821	-0.036473	2.152478
178.996924	1409.388291	18.204826	-0.036501	2.147265
178.897937	1401.460476	18.209831	-0.036478	2.142042
178.758887	1393.557084	18.214835	-0.036447	2.136820
178.704371	1385.603153	18.219840	-0.036433	2.131558
178.610909	1377.661536	18.224845	-0.036411	2.126289
178.580022	1369.745666	18.229850	-0.036401	2.121029
178.442673	1361.812565	18.234855	-0.036371	2.115734
178.327243	1353.837377	18.239859	-0.036345	2.110400
178.139114	1345.891527	18.244864	-0.036306	2.105065
178.246782	1337.933105	18.249869	-0.036321	2.099737
178.291610	1330.024286	18.254874	-0.036325	2.094423
177.941260	1322.101292	18.259879	-0.036256	2.089046
177.912403	1314.174572	18.264883	-0.036246	2.083685
178.161853	1306.216931	18.269888	-0.036288	2.078317
178.180223	1298.285096	18.274893	-0.036287	2.072929
178.062118	1290.363097	18.279898	-0.036261	2.067521
177.926113	1282.435294	18.284903	-0.036231	2.062092
177.916960	1274.522405	18.289907	-0.036225	2.056672
177.718667	1266.606306	18.294912	-0.036184	2.051217
177.581190	1258.672360	18.299917	-0.036154	2.045740
177.544884	1250.763167	18.304922	-0.036143	2.040277
177.649180	1242.810117	18.309927	-0.036158	2.034782
177.379656	1234.893293	18.314931	-0.036103	2.029260
177.137394	1226.979400	18.319936	-0.036054	2.023727
177.185404	1219.029933	18.324941	-0.036058	2.018185
177.489686	1211.065239	18.329946	-0.036110	2.012642
177.306811	1203.137691	18.334951	-0.036072	2.007060
177.495541	1195.208019	18.339955	-0.036103	2.001500
177.060739	1187.356522	18.344960	-0.036017	1.995914
177.137095	1179.399814	18.349965	-0.036027	1.990292
177.188078	1171.468834	18.354970	-0.036032	1.984669
177.070035	1163.566607	18.359975	-0.036006	1.979033
176.938999	1155.670984	18.364979	-0.035977	1.973384
177.140129	1147.694202	18.369984	-0.036010	1.967696
176.876645	1139.814557	18.374989	-0.035957	1.962012
176.811626	1131.919980	18.379994	-0.035940	1.956321
176.652398	1123.965379	18.384999	-0.035906	1.950561
176.675396	1116.024878	18.390003	-0.035906	1.944813
176.876100	1108.079794	18.395008	-0.035939	1.939065
176.545484	1100.207238	18.400013	-0.035873	1.933294
176.484468	1092.280467	18.405018	-0.035858	1.927495
176.537312	1084.349534	18.410023	-0.035863	1.921689
176.641633	1076.441710	18.415027	-0.035878	1.915888
176.489087	1068.542884	18.420032	-0.035845	1.910047
176.352956	1060.639905	18.425037	-0.035816	1.904187
176.147345	1052.760105	18.430042	-0.035773	1.898318
176.081663	1044.837695	18.435047	-0.035756	1.892415
176.123705	1036.916544	18.440051	-0.035760	1.886507
176.167754	1029.005884	18.445056	-0.035764	1.880588
176.010614	1021.121052	18.450061	-0.035730	1.874647
175.989048	1013.184370	18.455066	-0.035722	1.868664
175.810139	1005.287650	18.460071	-0.035684	1.862673
175.737435	997.399376	18.465075	-0.035666	1.856682
175.603343	989.493972	18.470080	-0.035637	1.850651
175.790146	981.549676	18.475085	-0.035667	1.844608
175.617905	973.701607	18.480090	-0.035631	1.838577
175.487418	965.799163	18.485095	-0.035602	1.832489
175.473038	957.882740	18.490099	-0.035595	1.826384
175.395366	949.995463	18.495104	-0.035576	1.820273
175.322786	942.113030	18.500109	-0.035558	1.814146
175.490356	934.177319	18.505114	-0.035585	1.807986
175.372045	926.295142	18.510119	-0.035559	1.801812
175.172781	918.446821	18.515123	-0.035517	1.795633
175.022086	910.494552	18.520128	-0.035485	1.789357
175.077788	902.577879	18.525133	-0.035491	1.783113
175.123756	894.695268	18.530138	-0.035495	1.776872
175.018674	886.794607	18.535143	-0.035471	1.770576
174.767182	878.950578	18.540147	-0.035420	1.764285
174.791923	871.065924	18.545152	-0.035420	1.757973
174.482933	863.212424	18.550157	-0.035358	1.751622
174.612063	855.293615	18.555162	-0.035378	1.745249
174.627488	847.402311	18.560167	-0.035377	1.738862
174.623221	839.530753	18.565171	-0.035371	1.732464
174.576711	831.632395	18.570176	-0.035358	1.726015
174.564559	823.768226	18.575181	-0.035352	1.719575
174.481876	815.908937	18.580186	-0.035332	1.713105
174.263560	808.021229	18.585191	-0.035287	1.706570
174.272853	800.145287	18.590195	-0.035285	1.700049
174.304156	792.268284	18.595200	-0.035286	1.693505
174.051844	784.404144	18.600205	-0.035235	1.686908
174.094537	776.536512	18.605210	-0.035238	1.680322
174.025260	768.672181	18.610215	-0.035221	1.673698
174.067071	760.787047	18.615219	-0.035224	1.667045
173.749229	752.966185	18.620224	-0.035161	1.660371
173.903261	745.073401	18.625229	-0.035185	1.653673
173.855401	737.208994	18.630234	-0.035172	1.646945
173.541017	729.380737	18.635239	-0.035109	1.640183
173.380066	721.547864	18.640243	-0.035075	1.633410
173.379928	713.615856	18.645248	-0.035071	1.626546
173.189767	705.778857	18.650253	-0.035031	1.619709
173.347854	697.906602	18.655258	-0.035056	1.612860
173.169096	690.049079	18.660263	-0.035018	1.605948
173.238329	682.203537	18.665267	-0.035027	1.599052
173.092343	674.376620	18.670272	-0.034995	1.592111
173.150391	666.500897	18.675277	-0.035002	1.585126
173.088882	658.677446	18.680282	-0.034986	1.578140
172.862040	650.852897	18.685287	-0.034939	1.571097
173.041254	642.977397	18.690291	-0.034969	1.564036
172.972489	635.157481	18.695296	-0.034951	1.556957
172.907491	627.309402	18.700301	-0.034935	1.549821
172.764414	619.501070	18.705306	-0.034904	1.542676
172.758571	611.649280	18.710311	-0.034899	1.535479
172.740118	603.815132	18.715315	-0.034891	1.528262
172.565793	596.016017	18.720320	-0.034854	1.521020
172.484919	588.208783	18.725325	-0.034835	1.513749
172.337140	580.392793	18.730330	-0.034803	1.506425
172.238133	572.571927	18.735335	-0.034780	1.499068
172.060158	564.775146	18.740339	-0.034743	1.491686
172.083294	556.937519	18.745344	-0.034743	1.484259
172.056078	549.136619	18.750349	-0.034733	1.476822
171.965767	541.293924	18.755354	-0.034712	1.469297
171.774905	533.492715	18.760359	-0.034672	1.461758
171.797394	525.686505	18.765363	-0.034672	1.454208
171.794728	517.866250	18.770368	-0.034667	1.446602
171.915689	510.058525	18.775373	-0.034686	1.438987
171.771778	502.289947	18.780378	-0.034655	1.431327
171.464684	494.530740	18.785383	-0.034593	1.423609
171.360489	486.758870	18.790387	-0.034570	1.415870
171.390785	478.948819	18.795392	-0.034571	1.408071
171.171299	471.196770	18.800397	-0.034526	1.400247
171.053918	463.438455	18.805402	-0.034500	1.392389
171.131650	455.604697	18.810407	-0.034510	1.384442
170.988372	447.865069	18.815411	-0.034479	1.376508
170.956436	440.080567	18.820416	-0.034469	1.368501
170.888114	432.317484	18.825421	-0.034452	1.360463
170.798117	424.579605	18.830426	-0.034431	1.352400
170.604471	416.825147	18.835431	-0.034390	1.344253
170.663571	409.071710	18.840435	-0.034397	1.336101
170.509204	401.333874	18.845440	-0.034364	1.327879
170.420193	393.594967	18.850445	-0.034343	1.319615
170.381065	385.795591	18.855450	-0.034332	1.311243
170.131450	378.021450	18.860455	-0.034281	1.302807
170.152040	370.297601	18.865459	-0.034280	1.294419
169.977753	362.584710	18.870464	-0.034244	1.285954
169.909119	354.881140	18.875469	-0.034227	1.277461
169.759909	347.181874	18.880474	-0.034195	1.268902
169.554619	339.494569	18.885479	-0.034152	1.260287
169.456670	331.805448	18.890483	-0.034130	1.251631
169.523491	324.080386	18.895488	-0.034138	1.242906
169.646413	316.359546	18.900493	-0.034157	1.234135
169.314656	308.704448	18.905498	-0.034091	1.225288
169.303503	301.011275	18.910503	-0.034084	1.216395
169.431903	293.305012	18.915507	-0.034104	1.207450
169.325713	285.661279	18.920512	-0.034080	1.198464
169.023745	278.031725	18.925517	-0.034020	1.189388
169.025469	270.372181	18.930522	-0.034016	1.180267
168.893740	262.727208	18.935527	-0.033987	1.171066
168.813996	255.099024	18.940531	-0.033968	1.161823
168.714825	247.463410	18.945536	-0.033945	1.152493
168.645894	239.803169	18.950541	-0.033928	1.143062
168.471261	232.211954	18.955546	-0.033892	1.133617
168.207462	224.616901	18.960551	-0.033838	1.124067
168.301312	216.998416	18.965555	-0.033852	1.114484
168.068107	209.423765	18.970560	-0.033804	1.104802
167.831771	201.863967	18.975565	-0.033756	1.095053
168.035938	194.243146	18.980570	-0.033790	1.085236
167.601066	186.737277	18.985575	-0.033705	1.075335
167.420931	179.179775	18.990579	-0.033667	1.065331
167.475338	171.606874	18.995584	-0.033673	1.055267
167.504201	164.049064	19.000589	-0.033674	1.045120
167.152536	156.583980	19.005594	-0.033605	1.034910
166.951033	149.075945	19.010599	-0.033563	1.024574
166.843500	141.583837	19.015603	-0.033539	1.014179
166.675783	134.104989	19.020608	-0.033504	1.003679
166.238036	126.675639	19.025613	-0.033418	0.993072
166.263562	119.158204	19.030618	-0.033419	0.982339
165.801356	111.759690	19.035623	-0.033329	0.971537
165.327169	104.382313	19.040627	-0.033236	0.960642
164.928891	97.001386	19.045632	-0.033158	0.949635
164.603027	89.612596	19.050637	-0.033093	0.938507
164.191176	82.258536	19.055642	-0.033013	0.927275
163.606093	74.951605	19.060647	-0.032900	0.915930
163.134182	67.620076	19.065651	-0.032808	0.904436
162.363282	60.599444	19.070656	-0.032661	0.893201