Thu Mar 11 18:01:17 2021

Number of Points = 3621
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.229960	0.108007	0.000000	0.000118	0.726761

0.538535	0.059191	0.005005	0.000060	0.726774
0.429584	0.074094	0.010010	0.000080	0.726765
0.601466	0.049650	0.015014	0.000048	0.726778
0.750026	0.020115	0.020019	0.000020	0.726773
0.737115	0.023764	0.025024	0.000022	0.726776
0.588946	0.047648	0.030029	0.000049	0.726772
0.599790	-0.089281	0.035034	0.000047	0.726509
0.798857	-0.144041	0.040038	0.000010	0.726472
0.463123	-0.091606	0.045043	0.000072	0.726458
0.267415	-0.058538	0.050048	0.000108	0.726455
0.581383	-0.109038	0.055053	0.000049	0.726467
0.504531	-0.100646	0.060058	0.000063	0.726457
0.380404	-0.077361	0.065062	0.000086	0.726460
0.377429	-0.080400	0.070067	0.000086	0.726454
0.622458	-0.122067	0.075072	0.000040	0.726458
0.432803	-0.086678	0.080077	0.000075	0.726462
0.443374	-0.091249	0.085082	0.000073	0.726457
0.699495	-0.131132	0.090086	0.000025	0.726469
0.428473	-0.225386	0.095091	0.000075	0.726191
0.070285	-0.190134	0.100096	0.000141	0.726136
0.368685	-0.239025	0.105101	0.000085	0.726145
0.577307	-0.277571	0.110106	0.000046	0.726143
0.242140	-0.217758	0.115110	0.000108	0.726144
0.414834	-0.247790	0.120115	0.000076	0.726146
0.587245	-0.307668	0.125120	0.000043	0.726090
0.341794	-0.364807	0.130125	0.000089	0.725894
0.303662	-0.363503	0.135130	0.000096	0.725883
0.776318	-0.442458	0.140134	0.000007	0.725894
0.749701	-0.441366	0.145139	0.000012	0.725888
0.411495	-0.452844	0.150144	0.000074	0.725748
0.473761	-0.563715	0.155149	0.000063	0.725554
0.533316	-0.578401	0.160154	0.000051	0.725547
0.359405	-0.547332	0.165158	0.000083	0.725548
0.311323	-0.568375	0.170163	0.000092	0.725490
0.362484	-0.710927	0.175168	0.000082	0.725230
0.175573	-0.678302	0.180173	0.000116	0.725229
-0.182728	-0.622111	0.185178	0.000183	0.725215
0.137313	-0.704842	0.190182	0.000123	0.725166
0.301567	-0.869463	0.195187	0.000092	0.724901
0.031051	-0.822711	0.200192	0.000142	0.724899
0.123557	-0.838352	0.205197	0.000125	0.724902
0.498631	-1.011138	0.210202	0.000054	0.724695
0.515352	-1.055808	0.215206	0.000051	0.724614
0.209798	-1.004054	0.220211	0.000108	0.724609
0.221920	-1.114176	0.225216	0.000105	0.724399
0.302070	-1.189417	0.230221	0.000090	0.724280
-0.108045	-1.123869	0.235226	0.000166	0.724266
0.204851	-1.271465	0.240230	0.000107	0.724087
0.063220	-1.309547	0.245235	0.000133	0.723963
-0.427405	-1.225596	0.250240	0.000224	0.723957
-0.430663	-1.338737	0.255245	0.000225	0.723735
-0.321369	-1.407879	0.260250	0.000204	0.723639
-0.318661	-1.405704	0.265254	0.000203	0.723644
-0.608304	-1.484809	0.270259	0.000257	0.723389
-0.267143	-1.565231	0.275264	0.000193	0.723351
0.306504	-1.696561	0.280269	0.000086	0.723294
-0.113733	-1.764769	0.285274	0.000164	0.723015
-0.553011	-1.686727	0.290278	0.000245	0.723015
-0.581196	-1.797191	0.295283	0.000250	0.722789
-0.960887	-1.776858	0.300288	0.000321	0.722697
-0.842844	-1.814833	0.305293	0.000298	0.722664
-0.913596	-1.952294	0.310298	0.000311	0.722371
-1.061204	-1.922087	0.315302	0.000338	0.722379
-1.555486	-1.922346	0.320307	0.000430	0.722206
-1.905017	-1.925982	0.325312	0.000495	0.722078
-2.101957	-1.890172	0.330317	0.000531	0.722080
-2.608903	-1.927787	0.335322	0.000625	0.721829
-3.438319	-1.819320	0.340326	0.000779	0.721753
-3.514410	-1.808286	0.345331	0.000793	0.721748
-3.201366	-1.919451	0.350336	0.000734	0.721640
-3.764835	-1.919720	0.355341	0.000839	0.721443
-4.235515	-1.840684	0.360346	0.000926	0.721434
-4.248366	-1.836462	0.365350	0.000928	0.721439
-4.117136	-1.975607	0.370355	0.000904	0.721212
-5.187015	-1.831741	0.375360	0.001102	0.721121
-4.981298	-1.863822	0.380365	0.001064	0.721130
-5.005705	-1.864489	0.385370	0.001068	0.721121
-5.505871	-1.853849	0.390374	0.001161	0.720967
-6.183913	-1.775970	0.395379	0.001286	0.720884
-5.841356	-1.838848	0.400384	0.001222	0.720881
-5.516040	-1.894133	0.405389	0.001162	0.720887
-6.284461	-1.770362	0.410394	0.001304	0.720862
-6.743670	-1.849117	0.415398	0.001389	0.720546
-6.445019	-1.904257	0.420403	0.001333	0.720543
-7.218454	-1.769828	0.425408	0.001477	0.720537
-6.804031	-1.838169	0.430413	0.001400	0.720549
-6.822036	-1.839972	0.435418	0.001403	0.720539
-7.098707	-1.949058	0.440422	0.001454	0.720228
-7.831797	-1.822087	0.445427	0.001590	0.720222
-8.295762	-1.739792	0.450432	0.001676	0.720222
-7.476515	-1.882529	0.455437	0.001523	0.720229
-7.894663	-1.812119	0.460442	0.001601	0.720221
-8.212027	-1.824930	0.465446	0.001659	0.720086
-8.663714	-1.840232	0.470451	0.001743	0.719898
-8.482420	-1.873997	0.475456	0.001709	0.719895
-8.953001	-1.785094	0.480461	0.001796	0.719906
-8.939133	-1.792925	0.485466	0.001793	0.719896
-8.470412	-1.874075	0.490470	0.001706	0.719901
-9.067470	-1.813870	0.495475	0.001817	0.719811
-9.677616	-1.811762	0.500480	0.001930	0.719602
-8.906910	-1.947289	0.505485	0.001786	0.719606
-9.730733	-1.804823	0.510490	0.001939	0.719598
-9.893103	-1.773781	0.515494	0.001969	0.719603
-9.538109	-1.839273	0.520499	0.001902	0.719599
-9.731889	-1.824773	0.525504	0.001938	0.719560
-10.337051	-1.863729	0.530509	0.002051	0.719272
-10.632785	-1.814833	0.535514	0.002105	0.719265
-10.761846	-1.788972	0.540518	0.002129	0.719271
-10.564295	-1.825039	0.545523	0.002092	0.719270
-10.904839	-1.767213	0.550528	0.002155	0.719265
-10.588214	-1.821676	0.555533	0.002096	0.719270
-10.618166	-1.850195	0.560538	0.002101	0.719204
-11.556978	-1.806704	0.565542	0.002275	0.718960
-11.339825	-1.846342	0.570547	0.002234	0.718959
-11.431241	-1.831894	0.575552	0.002251	0.718956
-11.407324	-1.831261	0.580557	0.002246	0.718966
-11.661433	-1.791240	0.585562	0.002293	0.718957
-11.486618	-1.820173	0.590566	0.002260	0.718962
-11.478252	-1.877574	0.595571	0.002259	0.718852
-12.761743	-1.755188	0.600576	0.002497	0.718643
-12.188197	-1.855652	0.605581	0.002390	0.718647
-12.406513	-1.821133	0.610586	0.002430	0.718639
-12.767195	-1.753744	0.615590	0.002497	0.718646
-12.377089	-1.824661	0.620595	0.002424	0.718644
-12.600000	-1.786119	0.625600	0.002465	0.718642
-12.539473	-1.807392	0.630605	0.002454	0.718622
-13.266205	-1.816305	0.635610	0.002589	0.718350
-13.112886	-1.838685	0.640614	0.002560	0.718360
-13.368087	-1.795539	0.645619	0.002607	0.718356
-13.673947	-1.742539	0.650624	0.002664	0.718354
-13.338244	-1.798826	0.655629	0.002601	0.718361
-13.342686	-1.802752	0.660634	0.002601	0.718353
-13.248225	-1.816586	0.665638	0.002583	0.718359
-14.050278	-1.833009	0.670643	0.002732	0.718045
-14.517307	-1.764102	0.675648	0.002819	0.718018
-14.403315	-1.781456	0.680653	0.002797	0.718024
-14.346579	-1.796554	0.685658	0.002786	0.718015
-14.392948	-1.786492	0.690662	0.002795	0.718019
-14.402652	-1.785172	0.695667	0.002796	0.718019
-14.792235	-1.718286	0.700672	0.002868	0.718015
-14.326362	-1.831539	0.705677	0.002781	0.717956
-15.259880	-1.794161	0.710682	0.002955	0.717702
-15.300954	-1.785279	0.715686	0.002962	0.717705
-15.633975	-1.725622	0.720691	0.003024	0.717707
-15.295829	-1.789340	0.725696	0.002960	0.717700
-15.045038	-1.831576	0.730701	0.002913	0.717706
-15.750693	-1.710719	0.735706	0.003044	0.717697
-15.398476	-1.770586	0.740710	0.002978	0.717703
-15.289204	-1.890631	0.745715	0.002958	0.717505
-16.639804	-1.716237	0.750720	0.003209	0.717375
-16.017899	-1.824302	0.755725	0.003093	0.717381
-16.214763	-1.793356	0.760730	0.003129	0.717374
-16.445765	-1.749579	0.765734	0.003172	0.717379
-16.179055	-1.797455	0.770739	0.003122	0.717379
-16.218658	-1.793257	0.775744	0.003129	0.717374
-16.048036	-1.886219	0.780749	0.003097	0.717251
-17.383308	-1.735636	0.785754	0.003345	0.717079
-16.926734	-1.813939	0.790758	0.003260	0.717086
-16.996909	-1.802558	0.795763	0.003272	0.717084
-17.359116	-1.742158	0.800768	0.003339	0.717077
-16.940399	-1.812534	0.805773	0.003261	0.717086
-17.206593	-1.768724	0.810778	0.003310	0.717079
-17.152671	-1.816059	0.815782	0.003300	0.717005
-17.848027	-1.820401	0.820787	0.003429	0.716752
-17.775747	-1.834987	0.825792	0.003415	0.716750
-17.967694	-1.796709	0.830797	0.003451	0.716758
-18.272787	-1.747820	0.835802	0.003507	0.716748
-17.753861	-1.837194	0.840806	0.003410	0.716755
-17.905075	-1.811535	0.845811	0.003438	0.716753
-18.203223	-1.778237	0.850816	0.003493	0.716714
-18.549506	-1.851088	0.855821	0.003557	0.716449
-18.784634	-1.814067	0.860826	0.003601	0.716440
-19.066207	-1.759747	0.865830	0.003653	0.716449
-18.972536	-1.777748	0.870835	0.003635	0.716447
-19.002522	-1.776245	0.875840	0.003640	0.716440
-18.594383	-1.841985	0.880845	0.003564	0.716454
-18.893038	-1.793845	0.885850	0.003619	0.716445
-19.506026	-1.841592	0.890854	0.003733	0.716135
-19.645604	-1.818870	0.895859	0.003759	0.716131
-20.281498	-1.707028	0.900864	0.003877	0.716129
-19.513622	-1.839377	0.905869	0.003733	0.716138
-19.622558	-1.827197	0.910874	0.003753	0.716125
-19.945272	-1.767006	0.915878	0.003813	0.716131
-19.666989	-1.818721	0.920883	0.003761	0.716127
-20.025238	-1.858641	0.925888	0.003827	0.715922
-20.194046	-1.846664	0.930893	0.003858	0.715887
-20.507415	-1.796487	0.935898	0.003916	0.715877
-20.455960	-1.802518	0.940902	0.003906	0.715883
-20.296494	-1.831334	0.945907	0.003876	0.715883
-20.408935	-1.813012	0.950912	0.003897	0.715881
-20.529176	-1.862297	0.955917	0.003919	0.715741
-21.698797	-1.754547	0.960922	0.004136	0.715542
-21.332164	-1.816017	0.965926	0.004068	0.715551
-21.287613	-1.824638	0.970931	0.004059	0.715550
-21.667129	-1.760706	0.975936	0.004129	0.715543
-21.274810	-1.826634	0.980941	0.004056	0.715552
-21.758905	-1.744348	0.985946	0.004146	0.715545
-21.723260	-1.775591	0.990950	0.004139	0.715496
-21.898101	-1.876418	0.995955	0.004171	0.715235
-22.406730	-1.788970	1.000960	0.004265	0.715229
-22.522066	-1.763914	1.005965	0.004287	0.715239
-22.238818	-1.819386	1.010970	0.004233	0.715229
-22.206438	-1.822533	1.015974	0.004227	0.715235
-22.490508	-1.774382	1.020979	0.004280	0.715231
-22.569209	-1.779302	1.025984	0.004294	0.715194
-22.847589	-1.870946	1.030989	0.004346	0.714915
-23.324118	-1.790944	1.035994	0.004434	0.714906
-23.551345	-1.747097	1.040998	0.004476	0.714913
-22.897261	-1.864857	1.046003	0.004354	0.714911
-23.336245	-1.790207	1.051008	0.004435	0.714905
-23.622062	-1.735882	1.056013	0.004488	0.714912
-23.356221	-1.788999	1.061018	0.004438	0.714901
-23.632527	-1.864793	1.066022	0.004489	0.714654
-24.172833	-1.790252	1.071027	0.004589	0.714611
-24.484749	-1.737214	1.076032	0.004647	0.714607
-23.886669	-1.840400	1.081037	0.004536	0.714614
-24.410319	-1.752746	1.086042	0.004633	0.714604
-24.460221	-1.740137	1.091046	0.004642	0.714612
-23.875801	-1.846864	1.096051	0.004532	0.714607
-24.499861	-1.844104	1.101056	0.004648	0.714393
-25.392455	-1.739994	1.106061	0.004814	0.714284
-25.098114	-1.799404	1.111066	0.004759	0.714271
-24.853544	-1.840163	1.116070	0.004713	0.714277
-25.364514	-1.750598	1.121075	0.004808	0.714275
-25.257646	-1.771579	1.126080	0.004788	0.714272
-24.856839	-1.837344	1.131085	0.004713	0.714284
-25.231737	-1.825967	1.136090	0.004782	0.714174
-26.253793	-1.746336	1.141094	0.004972	0.713971
-25.516944	-1.878455	1.146099	0.004835	0.713970
-26.145095	-1.767658	1.151104	0.004951	0.713969
-26.212514	-1.754012	1.156109	0.004963	0.713973
-25.905116	-1.812841	1.161114	0.004906	0.713965
-25.999298	-1.791285	1.166118	0.004923	0.713975
-25.965297	-1.831095	1.171123	0.004916	0.713909
-26.870983	-1.800890	1.176128	0.005085	0.713649
-26.473513	-1.865912	1.181133	0.005010	0.713661
-27.246877	-1.733205	1.186138	0.005154	0.713652
-27.128603	-1.753861	1.191142	0.005132	0.713653
-26.626559	-1.843325	1.196147	0.005038	0.713654
-26.945019	-1.789978	1.201152	0.005097	0.713648
-26.942816	-1.790426	1.206157	0.005096	0.713648
-27.670894	-1.808685	1.211162	0.005231	0.713355
-27.726989	-1.797138	1.216166	0.005241	0.713358
-27.943020	-1.758624	1.221171	0.005281	0.713359
-27.865890	-1.775757	1.226176	0.005266	0.713353
-27.535440	-1.830177	1.231181	0.005205	0.713362
-27.817946	-1.784096	1.236186	0.005257	0.713355
-28.005030	-1.747915	1.241190	0.005291	0.713361
-27.912445	-1.883460	1.246195	0.005274	0.713125
-28.912733	-1.758948	1.251200	0.005460	0.713019
-28.417211	-1.843881	1.256205	0.005367	0.713026
-28.522938	-1.830393	1.261210	0.005386	0.713016
-28.607685	-1.812760	1.266214	0.005402	0.713022
-28.589600	-1.816744	1.271219	0.005398	0.713021
-29.031606	-1.741497	1.276224	0.005480	0.713014
-28.943942	-1.868107	1.281229	0.005463	0.712794
-29.582514	-1.800252	1.286234	0.005582	0.712703
-29.677078	-1.782949	1.291238	0.005599	0.712705
-29.491446	-1.813650	1.296243	0.005564	0.712710
-29.806469	-1.761652	1.301248	0.005623	0.712703
-29.842546	-1.750771	1.306253	0.005629	0.712712
-29.879858	-1.749824	1.311258	0.005636	0.712702
-29.682980	-1.835761	1.316262	0.005599	0.712601
-30.518581	-1.794817	1.321267	0.005754	0.712387
-30.609722	-1.783257	1.326272	0.005770	0.712378
-30.666696	-1.768459	1.331277	0.005781	0.712388
-30.466799	-1.807777	1.336282	0.005743	0.712381
-30.427641	-1.813596	1.341286	0.005735	0.712384
-30.626472	-1.777988	1.346291	0.005772	0.712385
-30.609424	-1.785157	1.351296	0.005769	0.712378
-31.065190	-1.846716	1.356301	0.005853	0.712094
-31.763077	-1.725943	1.361306	0.005983	0.712087
-31.707014	-1.734618	1.366310	0.005972	0.712091
-31.394265	-1.790637	1.371315	0.005913	0.712091
-31.960963	-1.692574	1.376320	0.006018	0.712086
-31.411350	-1.787195	1.381325	0.005916	0.712093
-31.414018	-1.791867	1.386330	0.005916	0.712083
-31.717923	-1.813902	1.391334	0.005972	0.711932
-32.743742	-1.718242	1.396339	0.006163	0.711759
-32.136982	-1.829353	1.401344	0.006050	0.711754
-32.228475	-1.808056	1.406349	0.006066	0.711764
-32.690479	-1.730250	1.411354	0.006152	0.711756
-32.209686	-1.814530	1.416358	0.006062	0.711759
-31.961232	-1.859133	1.421363	0.006016	0.711759
-32.689332	-1.783271	1.426368	0.006151	0.711653
-33.324189	-1.768352	1.431373	0.006269	0.711457
-33.048295	-1.822227	1.436378	0.006217	0.711449
-33.600308	-1.722392	1.441382	0.006319	0.711452
-33.496937	-1.740673	1.446387	0.006300	0.711453
-33.137860	-1.807688	1.451392	0.006233	0.711448
-33.271210	-1.781008	1.456397	0.006257	0.711454
-33.729747	-1.703112	1.461402	0.006342	0.711447
-33.558315	-1.864579	1.466406	0.006310	0.711187
-33.902638	-1.827489	1.471411	0.006374	0.711139
-34.539967	-1.715461	1.476416	0.006492	0.711137
-34.186159	-1.775006	1.481421	0.006426	0.711144
-34.232854	-1.771865	1.486426	0.006434	0.711135
-34.380993	-1.743685	1.491430	0.006461	0.711139
-34.179730	-1.779059	1.496435	0.006423	0.711140
-34.422398	-1.833481	1.501440	0.006468	0.710946
-35.017861	-1.763747	1.506445	0.006579	0.710874
-35.161695	-1.743176	1.511450	0.006605	0.710865
-34.898998	-1.786997	1.516454	0.006556	0.710871
-34.551153	-1.850486	1.521459	0.006491	0.710869
-35.003472	-1.773926	1.526464	0.006575	0.710862
-35.100048	-1.753333	1.531469	0.006592	0.710869
-35.347727	-1.872087	1.536474	0.006638	0.710544
-35.734703	-1.808184	1.541478	0.006710	0.710535
-36.157249	-1.733957	1.546483	0.006788	0.710534
-35.864738	-1.789228	1.551488	0.006733	0.710528
-35.489668	-1.851161	1.556493	0.006663	0.710538
-36.131263	-1.742978	1.561498	0.006782	0.710527
-36.079834	-1.751770	1.566502	0.006772	0.710528
-36.356792	-1.858427	1.571507	0.006824	0.710217
-36.800632	-1.783215	1.576512	0.006906	0.710210
-37.040731	-1.735680	1.581517	0.006950	0.710220
-36.501776	-1.835689	1.586522	0.006850	0.710213
-36.774203	-1.785674	1.591526	0.006900	0.710216
-37.132880	-1.722045	1.596531	0.006966	0.710217
-37.035256	-1.741335	1.601536	0.006948	0.710213
-36.753498	-1.913796	1.606541	0.006895	0.709970
-37.817016	-1.763908	1.611546	0.007093	0.709891
-37.866838	-1.753564	1.616550	0.007102	0.709895
-37.331785	-1.848194	1.621555	0.007002	0.709897
-37.597629	-1.804153	1.626560	0.007051	0.709891
-37.572504	-1.806150	1.631565	0.007046	0.709896
-37.690629	-1.788162	1.636570	0.007067	0.709891
-38.033215	-1.871971	1.641574	0.007131	0.709602
-38.426859	-1.805113	1.646579	0.007204	0.709596
-38.970168	-1.711894	1.651584	0.007305	0.709590
-38.141566	-1.856071	1.656589	0.007150	0.709597
-38.606142	-1.776025	1.661594	0.007236	0.709592
-38.877664	-1.727380	1.666598	0.007286	0.709593
-38.148047	-1.859224	1.671603	0.007150	0.709591
-38.909505	-1.890745	1.676608	0.007292	0.709257
-39.446901	-1.788630	1.681613	0.007391	0.709270
-39.548650	-1.775819	1.686618	0.007410	0.709260
-39.143663	-1.844933	1.691622	0.007334	0.709267
-39.205824	-1.834770	1.696627	0.007346	0.709266
-39.686152	-1.752732	1.701632	0.007435	0.709259
-39.121771	-1.881885	1.706637	0.007329	0.709203
-40.249602	-1.806142	1.711642	0.007539	0.708953
-40.289134	-1.797906	1.716646	0.007546	0.708956
-40.385472	-1.779741	1.721651	0.007563	0.708958
-40.441143	-1.775062	1.726656	0.007573	0.708948
-40.455647	-1.768285	1.731661	0.007576	0.708957
-40.501541	-1.763983	1.736666	0.007584	0.708950
-40.244508	-1.807043	1.741670	0.007536	0.708957
-40.533539	-1.886048	1.746675	0.007589	0.708696
-41.777231	-1.695580	1.751680	0.007820	0.708634
-41.186085	-1.796399	1.756685	0.007710	0.708644
-40.765861	-1.875756	1.761690	0.007632	0.708636
-41.460743	-1.750874	1.766694	0.007760	0.708638
-41.140520	-1.808004	1.771699	0.007701	0.708639
-41.084188	-1.821609	1.776704	0.007690	0.708632
-41.442731	-1.863660	1.781709	0.007756	0.708421
-42.232929	-1.761363	1.786714	0.007903	0.708344
-41.915912	-1.816483	1.791718	0.007844	0.708348
-42.008486	-1.798872	1.796723	0.007860	0.708350
-42.565127	-1.704548	1.801728	0.007964	0.708341
-42.019684	-1.798082	1.806733	0.007862	0.708349
-41.925573	-1.817445	1.811738	0.007844	0.708345
-42.660567	-1.805046	1.816742	0.007980	0.708108
-43.178235	-1.761387	1.821747	0.008076	0.708011
-42.783835	-1.835129	1.826752	0.008003	0.708005
-42.774468	-1.831444	1.831757	0.008001	0.708016
-43.399845	-1.724630	1.836762	0.008117	0.708008
-42.939167	-1.805124	1.841766	0.008031	0.708011
-42.784018	-1.832641	1.846771	0.008001	0.708012
-43.441249	-1.779124	1.851776	0.008123	0.707885
-43.936082	-1.780029	1.856781	0.008215	0.707707
-43.613487	-1.844124	1.861786	0.008155	0.707695
-44.067447	-1.762839	1.866790	0.008239	0.707696
-43.856768	-1.798698	1.871795	0.008199	0.707700
-43.515869	-1.861269	1.876800	0.008136	0.707697
-43.795812	-1.808472	1.881805	0.008187	0.707704
-44.150773	-1.814676	1.886810	0.008253	0.707565
-45.036416	-1.752256	1.891814	0.008418	0.707374
-44.522196	-1.842571	1.896819	0.008322	0.707378
-45.007142	-1.760468	1.901824	0.008412	0.707370
-44.693331	-1.811133	1.906829	0.008353	0.707381
-44.621027	-1.827696	1.911834	0.008339	0.707374
-45.016857	-1.755643	1.916838	0.008412	0.707378
-44.831817	-1.813653	1.921843	0.008378	0.707328
-45.350505	-1.847943	1.926848	0.008474	0.707075
-45.403441	-1.833201	1.931853	0.008483	0.707086
-46.110299	-1.710994	1.936858	0.008614	0.707079
-45.776792	-1.769683	1.941862	0.008552	0.707081
-45.259642	-1.861456	1.946867	0.008455	0.707083
-46.070759	-1.718955	1.951872	0.008606	0.707079
-45.796346	-1.765206	1.956877	0.008555	0.707085
-46.051993	-1.886479	1.961882	0.008602	0.706751
-46.723403	-1.764914	1.966886	0.008727	0.706755
-46.928870	-1.726443	1.971891	0.008764	0.706759
-46.361444	-1.832543	1.976896	0.008659	0.706750
-46.494011	-1.803453	1.981901	0.008683	0.706762
-46.885940	-1.738156	1.986906	0.008755	0.706753
-46.692441	-1.771890	1.991910	0.008719	0.706756
-46.425947	-1.930144	1.996915	0.008669	0.706534
-47.836668	-1.722932	2.001920	0.008931	0.706445

-47.430308	-1.797312	2.011917	0.008855	0.706443
-47.666147	-1.756282	2.021914	0.008898	0.706442
-47.582005	-1.769957	2.031910	0.008882	0.706446
-47.663713	-1.756091	2.041907	0.008897	0.706446
-47.703481	-1.750984	2.051904	0.008903	0.706443
-47.698454	-1.753434	2.061901	0.008902	0.706442
-47.680670	-1.755669	2.071898	0.008898	0.706445
-47.392636	-1.808295	2.081894	0.008843	0.706444
-47.525657	-1.786682	2.091891	0.008867	0.706441
-47.740690	-1.747883	2.101888	0.008907	0.706443
-47.644386	-1.766254	2.111885	0.008888	0.706442
-47.682272	-1.707771	2.121882	0.008894	0.706547
-46.653865	-1.789513	2.131878	0.008702	0.706752
-46.712769	-1.779050	2.141875	0.008713	0.706754
-46.823059	-1.759467	2.151872	0.008732	0.706755
-46.606713	-1.800091	2.161869	0.008691	0.706752
-46.920926	-1.718789	2.171866	0.008749	0.706804
-45.863529	-1.770078	2.181862	0.008552	0.707081
-45.822137	-1.776715	2.191859	0.008543	0.707084
-45.927091	-1.760263	2.201856	0.008562	0.707081
-45.708725	-1.800157	2.211853	0.008521	0.707080
-45.369230	-1.747761	2.221850	0.008457	0.707308
-45.021905	-1.776060	2.231846	0.008392	0.707377
-44.932826	-1.792442	2.241843	0.008374	0.707377
-45.008640	-1.780718	2.251840	0.008388	0.707375
-44.306859	-1.758756	2.261837	0.008256	0.707671
-44.179281	-1.768636	2.271834	0.008232	0.707698
-44.172511	-1.771515	2.281830	0.008230	0.707696
-44.242636	-1.710345	2.291827	0.008242	0.707795
-43.158647	-1.796059	2.301824	0.008040	0.708012
-43.137813	-1.800938	2.311821	0.008035	0.708011
-43.307389	-1.770867	2.321818	0.008066	0.708012
-42.903072	-1.756106	2.331814	0.007990	0.708187
-42.376061	-1.767635	2.341811	0.007891	0.708354
-42.350195	-1.774309	2.351808	0.007886	0.708351
-42.390255	-1.770130	2.361805	0.007893	0.708346
-41.902859	-1.728036	2.371802	0.007801	0.708606
-41.574569	-1.769298	2.381798	0.007739	0.708642
-41.461959	-1.790496	2.391795	0.007718	0.708641
-41.298423	-1.754591	2.401792	0.007686	0.708773
-40.657499	-1.778892	2.411789	0.007566	0.708954
-40.662485	-1.777960	2.421786	0.007567	0.708955
-40.663314	-1.778667	2.431782	0.007566	0.708955
-40.110694	-1.736206	2.441779	0.007463	0.709239
-39.905651	-1.760599	2.451776	0.007424	0.709264
-39.759266	-1.788832	2.461773	0.007396	0.709261
-39.676242	-1.724688	2.471770	0.007380	0.709420
-38.834002	-1.788214	2.481766	0.007222	0.709595
-38.926215	-1.771541	2.491763	0.007239	0.709597
-38.967460	-1.764264	2.501760	0.007246	0.709598
-38.399192	-1.721833	2.511757	0.007139	0.709887
-38.183021	-1.760079	2.521754	0.007098	0.709888
-38.093837	-1.774483	2.531750	0.007081	0.709893
-37.874079	-1.703235	2.541747	0.007039	0.710115
-37.379415	-1.742034	2.551744	0.006946	0.710215
-37.562281	-1.712529	2.561741	0.006980	0.710210
-37.205462	-1.707589	2.571738	0.006913	0.710348
-36.316934	-1.775400	2.581734	0.006747	0.710530
-36.464092	-1.749482	2.591731	0.006773	0.710531
-36.337081	-1.773480	2.601728	0.006749	0.710530
-35.815473	-1.703858	2.611725	0.006651	0.710856
-35.508714	-1.753154	2.621722	0.006593	0.710868
-35.624638	-1.733626	2.631718	0.006614	0.710867
-35.274142	-1.726549	2.641715	0.006548	0.711007
-34.711855	-1.761819	2.651712	0.006443	0.711138
-34.850504	-1.738789	2.661709	0.006468	0.711136
-34.709246	-1.747624	2.671706	0.006441	0.711170
-33.968403	-1.737912	2.681702	0.006302	0.711454
-33.709034	-1.784868	2.691699	0.006253	0.711454
-33.917268	-1.750106	2.701696	0.006291	0.711450
-33.471376	-1.723440	2.711693	0.006208	0.711663
-33.014904	-1.757504	2.721690	0.006122	0.711759
-33.162265	-1.731631	2.731686	0.006149	0.711759
-32.970435	-1.721589	2.741683	0.006112	0.711849
-32.096279	-1.758934	2.751680	0.005949	0.712086
-32.246877	-1.733583	2.761677	0.005976	0.712084
-32.149325	-1.750762	2.771674	0.005957	0.712086
-31.579959	-1.719356	2.781670	0.005851	0.712352
-31.348696	-1.743490	2.791667	0.005807	0.712387
-31.132253	-1.783383	2.801664	0.005766	0.712386
-31.435182	-1.660851	2.811661	0.005822	0.712524
-30.343506	-1.764581	2.821658	0.005618	0.712706
-30.632424	-1.710936	2.831654	0.005671	0.712712
-30.565607	-1.695199	2.841651	0.005658	0.712768
-29.891069	-1.688677	2.851648	0.005531	0.713022
-29.617706	-1.737729	2.861645	0.005480	0.713022
-29.673017	-1.728298	2.871642	0.005489	0.713023
-29.103175	-1.684962	2.881638	0.005383	0.713312
-28.697220	-1.733081	2.891635	0.005306	0.713362
-28.713757	-1.732916	2.901632	0.005309	0.713357
-28.733093	-1.682823	2.911629	0.005312	0.713452
-27.946438	-1.724288	2.921626	0.005164	0.713649
-28.049273	-1.706350	2.931622	0.005183	0.713650
-27.775373	-1.754906	2.941619	0.005131	0.713651
-27.332857	-1.678796	2.951616	0.005048	0.713961
-26.771809	-1.776582	2.961613	0.004943	0.713966
-27.022635	-1.731335	2.971610	0.004989	0.713969
-26.872742	-1.691055	2.981606	0.004960	0.714103
-26.011702	-1.754208	2.991603	0.004799	0.714284
-26.342072	-1.698408	3.001600	0.004860	0.714279
-26.233727	-1.714436	3.011597	0.004839	0.714287
-25.421349	-1.697617	3.021594	0.004687	0.714609
-25.267475	-1.726122	3.031590	0.004658	0.714608
-25.264529	-1.725929	3.041587	0.004657	0.714611
-25.136050	-1.660312	3.051584	0.004632	0.714788
-24.342374	-1.741059	3.061581	0.004484	0.714910
-24.601284	-1.695238	3.071578	0.004531	0.714910
-24.434766	-1.700596	3.081574	0.004500	0.714960
-23.592866	-1.714084	3.091571	0.004342	0.715232
-23.647348	-1.705392	3.101568	0.004352	0.715231
-23.552344	-1.724513	3.111565	0.004333	0.715228
-23.142573	-1.679880	3.121562	0.004256	0.715463
-22.802701	-1.697849	3.131558	0.004192	0.715549
-22.699450	-1.717887	3.141555	0.004172	0.715547
-22.742870	-1.659292	3.151552	0.004180	0.715649
-21.380508	-1.786724	3.161549	0.003925	0.715879
-21.772287	-1.716685	3.171546	0.003998	0.715880
-21.659134	-1.737107	3.181542	0.003976	0.715881
-21.341892	-1.728534	3.191539	0.003916	0.716011
-21.017595	-1.726452	3.201536	0.003855	0.716131
-20.947460	-1.741854	3.211533	0.003841	0.716127
-21.254141	-1.657821	3.221530	0.003898	0.716186
-20.079944	-1.736478	3.231526	0.003678	0.716446
-20.053647	-1.740322	3.241523	0.003673	0.716449
-20.314917	-1.694875	3.251520	0.003721	0.716448
-19.546656	-1.700537	3.261517	0.003577	0.716709
-19.446585	-1.697385	3.271514	0.003558	0.716752
-18.922926	-1.789427	3.281510	0.003460	0.716756
-19.280327	-1.658897	3.291507	0.003525	0.716889
-18.232624	-1.746325	3.301504	0.003330	0.717087
-18.392118	-1.721379	3.311501	0.003359	0.717081
-18.344244	-1.729855	3.321498	0.003349	0.717083
-17.669751	-1.720741	3.331494	0.003223	0.717340
-17.654990	-1.702570	3.341491	0.003219	0.717382
-17.384297	-1.753618	3.351488	0.003168	0.717378
-17.509358	-1.658405	3.361485	0.003191	0.717524
-16.805775	-1.693375	3.371482	0.003059	0.717703
-16.509867	-1.745672	3.381478	0.003003	0.717706
-16.658465	-1.714684	3.391475	0.003030	0.717716
-15.624619	-1.746823	3.401472	0.002837	0.718017
-15.708810	-1.731973	3.411469	0.002852	0.718018
-15.860710	-1.707120	3.421466	0.002880	0.718015
-15.576383	-1.677673	3.431462	0.002826	0.718175
-14.889767	-1.709251	3.441459	0.002697	0.718355
-14.822361	-1.720451	3.451456	0.002684	0.718358
-14.999582	-1.685430	3.461453	0.002717	0.718366
-13.871192	-1.746886	3.471450	0.002506	0.718643
-13.845864	-1.750115	3.481446	0.002500	0.718647
-14.166359	-1.693456	3.491443	0.002559	0.718647
-13.646307	-1.718984	3.501440	0.002462	0.718781
-13.176022	-1.713175	3.511437	0.002374	0.718959
-13.020929	-1.742764	3.521434	0.002344	0.718957
-12.892617	-1.763621	3.531430	0.002319	0.718962
-12.152076	-1.780400	3.541427	0.002181	0.719190
-11.987932	-1.769713	3.551424	0.002150	0.719270
-12.185748	-1.734745	3.561421	0.002186	0.719271
-11.915299	-1.784204	3.571418	0.002135	0.719270
-11.347299	-1.719412	3.581414	0.002028	0.719598
-11.135370	-1.754047	3.591411	0.001988	0.719606
-10.827624	-1.809949	3.601408	0.001930	0.719605
-11.228245	-1.705239	3.611405	0.002004	0.719672
-10.018499	-1.806206	3.621402	0.001778	0.719899
-10.115761	-1.787878	3.631398	0.001796	0.719902
-10.137443	-1.783486	3.641395	0.001799	0.719904
-9.571113	-1.801688	3.651392	0.001693	0.720068
-9.152005	-1.796866	3.661389	0.001614	0.720226
-9.083389	-1.810101	3.671386	0.001601	0.720225
-9.213870	-1.787326	3.681382	0.001624	0.720226
-8.590774	-1.802972	3.691379	0.001507	0.720415
-8.418871	-1.768379	3.701376	0.001475	0.720544
-8.432156	-1.768380	3.711373	0.001477	0.720541
-8.199207	-1.808696	3.721370	0.001432	0.720545
-7.410476	-1.779355	3.731366	0.001285	0.720880
-7.203849	-1.814188	3.741363	0.001246	0.720885
-7.296289	-1.799974	3.751360	0.001262	0.720882
-7.590976	-1.717806	3.761357	0.001316	0.720942
-6.613258	-1.801384	3.771354	0.001134	0.721121
-6.781301	-1.771761	3.781350	0.001164	0.721122
-6.656419	-1.793903	3.791347	0.001140	0.721123
-5.986474	-1.755029	3.801344	0.001015	0.721436
-5.829647	-1.783097	3.811341	0.000985	0.721437
-5.778987	-1.795004	3.821338	0.000975	0.721432
-5.559161	-1.737311	3.831334	0.000933	0.721624
-5.170816	-1.745635	3.841331	0.000860	0.721745
-4.847377	-1.803728	3.851328	0.000799	0.721745
-5.039210	-1.727310	3.861325	0.000834	0.721829
-4.136573	-1.764959	3.871322	0.000666	0.722072
-3.926808	-1.803009	3.881318	0.000626	0.722072
-4.400055	-1.718247	3.891315	0.000713	0.722075
-3.344326	-1.755999	3.901312	0.000516	0.722371
-3.822666	-1.671487	3.911309	0.000604	0.722371
-3.228565	-1.779363	3.921306	0.000493	0.722368
-3.300257	-1.649558	3.931302	0.000506	0.722599
-3.253215	-1.608094	3.941299	0.000496	0.722698
-2.558890	-1.732419	3.951296	0.000366	0.722698
-2.947209	-1.526781	3.961293	0.000438	0.722967
-1.903171	-1.691574	3.971290	0.000243	0.723010
-2.356737	-1.592947	3.981286	0.000327	0.723046
-1.608312	-1.571177	3.991283	0.000186	0.723351
-2.085482	-1.488114	4.001280	0.000275	0.723349
-2.085261	-1.417008	4.011277	0.000274	0.723490
-2.162338	-1.329293	4.021274	0.000287	0.723636
-1.934332	-1.301705	4.031270	0.000244	0.723771
-1.786369	-1.233599	4.041267	0.000216	0.723957
-1.143209	-1.278413	4.051264	0.000096	0.724095
-1.270699	-1.163778	4.061261	0.000119	0.724276
-1.022847	-1.143451	4.071258	0.000072	0.724404
-1.175609	-1.011897	4.081254	0.000099	0.724609
-1.330447	-0.897520	4.091251	0.000127	0.724781
-1.132867	-0.869435	4.101248	0.000090	0.724906
-1.364356	-0.668960	4.111245	0.000132	0.725218
-0.542695	-0.730866	4.121242	-0.000021	0.725385
-0.464593	-0.658423	4.131238	-0.000037	0.725555
-0.526816	-0.499737	4.141235	-0.000026	0.725844
-0.546209	-0.418687	4.151232	-0.000023	0.725997
-0.790267	-0.289022	4.161229	0.000022	0.726167
-0.355651	-0.213889	4.171226	-0.000060	0.726466
-0.353835	-0.097057	4.181222	-0.000061	0.726696
-0.113417	-0.020295	4.191219	-0.000107	0.726930
-0.019435	0.087221	4.201216	-0.000125	0.727174
0.000000	0.257793	4.211213	-0.000129	0.727514

0.046810	0.883879	4.216218	-0.000139	0.728750
0.276638	2.117474	4.221222	-0.000183	0.731227
0.853786	3.894772	4.226227	-0.000292	0.734864
1.616489	6.198423	4.231232	-0.000436	0.739556
2.414544	9.010695	4.236237	-0.000586	0.745199
3.894189	12.208364	4.241242	-0.000864	0.751755
4.675438	15.970247	4.246246	-0.001013	0.759076
5.477011	20.151241	4.251251	-0.001165	0.767109
6.865655	24.642100	4.256256	-0.001427	0.775815
8.179050	29.516891	4.261261	-0.001675	0.785094
9.428232	34.773788	4.266266	-0.001911	0.794925
11.030869	40.273850	4.271270	-0.002213	0.805174
12.505635	46.133224	4.276275	-0.002492	0.815878
13.353750	52.388451	4.281280	-0.002655	0.826932
14.438503	58.875894	4.286285	-0.002861	0.838303
15.989903	65.504207	4.291290	-0.003155	0.849893
17.006504	72.442183	4.296294	-0.003349	0.861681
17.967547	79.608701	4.301299	-0.003533	0.873664
19.148889	86.912541	4.306304	-0.003758	0.885766
19.870658	94.477038	4.311309	-0.003898	0.897989
20.642878	102.196876	4.316314	-0.004047	0.910302
21.448002	110.025609	4.321318	-0.004202	0.922627
21.894509	118.042912	4.326323	-0.004291	0.934980
22.590388	126.118049	4.331328	-0.004426	0.947323
23.142285	134.305304	4.336333	-0.004534	0.959635
23.938084	142.546347	4.341338	-0.004688	0.971932
24.415980	150.907865	4.346342	-0.004783	0.984168
25.056599	159.338802	4.351347	-0.004908	0.996392
25.798074	167.759170	4.356352	-0.005052	1.008478
26.399094	176.251899	4.361357	-0.005170	1.020486
26.962362	184.804815	4.366362	-0.005281	1.032429
27.637273	193.349612	4.371366	-0.005412	1.044249
28.505072	201.907474	4.376371	-0.005580	1.055999
28.963415	210.551455	4.381376	-0.005671	1.067640
29.623286	219.168036	4.386381	-0.005800	1.079165
30.582554	227.741606	4.391386	-0.005984	1.090579
31.101393	236.400205	4.396390	-0.006087	1.101885
31.576812	245.070702	4.401395	-0.006182	1.113082
32.170444	253.719863	4.406400	-0.006298	1.124167
32.396339	262.428218	4.411405	-0.006346	1.135137
33.287442	271.019779	4.416410	-0.006518	1.145999
34.396025	279.610188	4.421414	-0.006730	1.156803
34.884561	288.237379	4.426419	-0.006827	1.167422
35.257935	296.904924	4.431424	-0.006903	1.177971
35.483418	305.555914	4.436429	-0.006951	1.188375
36.098331	314.144930	4.441434	-0.007071	1.198694
36.790382	322.692492	4.446438	-0.007206	1.208892
37.502020	331.240184	4.451443	-0.007344	1.219008
38.269771	339.782036	4.456448	-0.007493	1.229045
38.777134	348.346403	4.461453	-0.007594	1.238975
38.905255	356.955334	4.466458	-0.007624	1.248804
39.212272	365.512487	4.471462	-0.007687	1.258531
39.637022	374.024328	4.476467	-0.007772	1.268156
40.263590	382.515132	4.481472	-0.007894	1.277722
40.679531	390.983011	4.486477	-0.007977	1.287153
41.303522	399.459364	4.491482	-0.008100	1.296562
41.732812	407.917863	4.496486	-0.008185	1.305848
42.214172	416.498346	4.501491	-0.008281	1.315209
43.081478	424.847359	4.506496	-0.008448	1.324326
43.557138	433.260130	4.511501	-0.008543	1.333378
43.979598	441.676901	4.516506	-0.008627	1.342363
44.657114	450.044311	4.521510	-0.008759	1.351282
45.268702	458.414702	4.526515	-0.008879	1.360133
45.753628	466.803529	4.531520	-0.008975	1.368924
46.304910	475.175661	4.536525	-0.009083	1.377653
47.126664	483.489963	4.541530	-0.009242	1.386314
47.484306	491.906917	4.546534	-0.009314	1.394946
47.650404	500.295927	4.551539	-0.009351	1.403465
48.162127	508.635470	4.556544	-0.009452	1.411941
48.762090	516.934493	4.561549	-0.009570	1.420339
49.291744	525.257394	4.566554	-0.009674	1.428701
49.430940	533.649460	4.571558	-0.009706	1.437018
49.877674	541.941164	4.576563	-0.009795	1.445238
50.380326	550.263891	4.581568	-0.009894	1.453451
50.566394	558.591105	4.586573	-0.009935	1.461571
51.368851	566.859922	4.591578	-0.010090	1.469688
51.610584	575.213594	4.596582	-0.010140	1.477753
52.145598	583.453592	4.601587	-0.010246	1.485712
52.753106	591.730152	4.606592	-0.010365	1.493674
53.148181	599.992904	4.611597	-0.010444	1.501547
53.727675	608.254884	4.616602	-0.010558	1.509407
54.010366	616.540181	4.621606	-0.010616	1.517203
54.532890	624.763260	4.626611	-0.010719	1.524937
55.470677	632.962166	4.631616	-0.010899	1.532672
55.546296	641.251273	4.636621	-0.010919	1.540322
56.109409	649.494707	4.641626	-0.011030	1.547965
56.608854	657.753068	4.646630	-0.011128	1.555574
56.770968	666.017295	4.651635	-0.011164	1.563102
57.165798	674.261872	4.656640	-0.011244	1.570609
57.593295	682.486704	4.661645	-0.011329	1.578068
57.945327	690.711778	4.666650	-0.011400	1.585481
58.384802	698.946470	4.671654	-0.011488	1.592881
59.033459	707.113183	4.676659	-0.011614	1.600215
59.601021	715.316825	4.681664	-0.011725	1.607537
60.071388	723.527864	4.686669	-0.011819	1.614819
60.864434	731.693589	4.691674	-0.011972	1.622073
61.421501	739.914789	4.696678	-0.012082	1.629310
61.808465	748.172597	4.701683	-0.012159	1.636523
62.338928	756.348734	4.706688	-0.012264	1.643653
62.854659	764.527499	4.711693	-0.012365	1.650753
63.280269	772.748751	4.716698	-0.012450	1.657846
63.574264	780.942189	4.721702	-0.012511	1.664868
63.875253	789.160439	4.726707	-0.012573	1.671881
64.330409	797.351552	4.731712	-0.012663	1.678864
64.546800	805.537017	4.736717	-0.012709	1.685780
65.171494	813.710856	4.741722	-0.012831	1.692712
65.677332	821.875262	4.746726	-0.012931	1.699593
66.031015	830.055357	4.751731	-0.013002	1.706438
66.677518	838.242428	4.756736	-0.013128	1.713300
66.760149	846.438490	4.761741	-0.013149	1.720069
67.292154	854.583984	4.766746	-0.013254	1.726828
67.686404	862.762367	4.771750	-0.013333	1.733569
68.155899	870.898858	4.776755	-0.013426	1.740260
68.847955	879.031567	4.781760	-0.013561	1.746950
69.037308	887.241504	4.786765	-0.013602	1.753613
69.504739	895.383763	4.791770	-0.013694	1.760231
69.859134	903.545758	4.796774	-0.013766	1.766826
70.268005	911.727023	4.801779	-0.013848	1.773419
70.501550	919.903029	4.806784	-0.013897	1.779961
71.116089	928.015914	4.811789	-0.014017	1.786476
71.798546	936.203884	4.816794	-0.014150	1.793035
72.010441	944.375355	4.821798	-0.014195	1.799499
72.261561	952.515200	4.826803	-0.014247	1.805920
72.535845	960.687107	4.831808	-0.014304	1.812346
72.692950	968.842404	4.836813	-0.014339	1.818722
72.989182	976.975062	4.841818	-0.014400	1.825075
73.635701	985.073352	4.846822	-0.014526	1.831421
73.825515	993.232474	4.851827	-0.014567	1.837738
74.163730	1001.370647	4.856832	-0.014636	1.844034
74.520306	1009.498650	4.861837	-0.014708	1.850303
75.018552	1017.627965	4.866842	-0.014806	1.856569
75.295780	1025.767459	4.871846	-0.014863	1.862795
75.603693	1033.919886	4.876851	-0.014926	1.869014
76.122826	1042.063827	4.881856	-0.015029	1.875230
76.514414	1050.166310	4.886861	-0.015107	1.881379
76.694174	1058.312299	4.891866	-0.015146	1.887517
77.099332	1066.450740	4.896870	-0.015227	1.893654
77.469542	1074.555053	4.901875	-0.015302	1.899743
77.958326	1082.667117	4.906880	-0.015399	1.905831
78.178767	1090.820046	4.911885	-0.015445	1.911899
78.649733	1098.930970	4.916890	-0.015539	1.917945
79.048001	1107.027962	4.921894	-0.015618	1.923954
79.418516	1115.138856	4.926899	-0.015693	1.929951
79.753280	1123.293738	4.931904	-0.015761	1.935958
79.977224	1131.407803	4.936909	-0.015808	1.941904
80.263861	1139.538400	4.941914	-0.015867	1.947850
80.661733	1147.702003	4.946918	-0.015947	1.953815
81.134521	1155.756239	4.951923	-0.016041	1.959690
81.535256	1163.846500	4.956928	-0.016121	1.965566
81.835599	1171.964803	4.961933	-0.016182	1.971433
82.323368	1180.067387	4.966938	-0.016279	1.977292
82.607647	1188.173778	4.971942	-0.016337	1.983115
82.793279	1196.309277	4.976947	-0.016378	1.988930
83.311232	1204.423780	4.981952	-0.016480	1.994749
83.732424	1212.487175	4.986957	-0.016564	2.000504
84.129064	1220.592851	4.991962	-0.016643	2.006270
84.399627	1228.731310	4.996966	-0.016699	2.012029
84.869113	1236.816060	5.001971	-0.016792	2.017755
85.183702	1244.930301	5.006976	-0.016857	2.023469
85.383092	1253.051603	5.011981	-0.016899	2.029159
85.777473	1261.188956	5.016986	-0.016978	2.034865
85.932313	1269.280465	5.021990	-0.017013	2.040499
86.083687	1277.377605	5.026995	-0.017047	2.046121
86.660791	1285.454421	5.032000	-0.017160	2.051756
86.885951	1293.555747	5.037005	-0.017207	2.057357
87.181697	1301.653320	5.042010	-0.017268	2.062947
87.577346	1309.740716	5.047014	-0.017347	2.068525
88.196005	1317.819807	5.052019	-0.017468	2.074105
88.538407	1325.908848	5.057024	-0.017537	2.079648
88.725547	1334.008521	5.062029	-0.017578	2.085169
89.217827	1342.105801	5.067034	-0.017675	2.090704
89.270994	1350.259960	5.072038	-0.017691	2.096219
89.538589	1358.340809	5.077043	-0.017746	2.101691
89.791815	1366.458975	5.082048	-0.017799	2.107173
90.054270	1374.591800	5.087053	-0.017853	2.112651
90.404634	1382.685353	5.092058	-0.017924	2.118097
90.750901	1390.731247	5.097062	-0.017994	2.123497
91.225216	1398.781591	5.102067	-0.018088	2.128898
91.580216	1406.882858	5.107072	-0.018160	2.134308
91.580647	1414.987841	5.112077	-0.018166	2.139672
91.880961	1423.073523	5.117082	-0.018227	2.145039
92.307688	1431.142148	5.122086	-0.018312	2.150394
92.350835	1439.269861	5.127091	-0.018326	2.155737
92.715932	1447.325097	5.132096	-0.018400	2.161050
92.955349	1455.389666	5.137101	-0.018450	2.166345
93.393936	1463.471696	5.142106	-0.018537	2.171656
93.710734	1471.555605	5.147110	-0.018602	2.176944
94.104167	1479.615789	5.152115	-0.018680	2.182211
94.423959	1487.716330	5.157120	-0.018746	2.187484
94.453508	1495.866860	5.162125	-0.018757	2.192750
94.911361	1503.923600	5.167130	-0.018848	2.197983
95.268759	1511.977835	5.172134	-0.018920	2.203192
95.469577	1520.048616	5.177139	-0.018963	2.208385
95.805241	1528.157689	5.182144	-0.019031	2.213602
96.051831	1536.214430	5.187149	-0.019082	2.218766
96.478092	1544.288969	5.192154	-0.019167	2.223945
96.613111	1552.392229	5.197158	-0.019198	2.229105
96.820779	1560.489410	5.202163	-0.019242	2.234254
97.217515	1568.550832	5.207168	-0.019322	2.239387
97.084832	1576.646720	5.212173	-0.019303	2.244482
97.502081	1584.712086	5.217178	-0.019386	2.249595
97.838474	1592.799900	5.222182	-0.019454	2.254703
97.907398	1600.872396	5.227187	-0.019473	2.259767
98.321453	1608.934909	5.232192	-0.019556	2.264843
98.526733	1617.027714	5.237197	-0.019599	2.269908
98.856174	1625.159742	5.242202	-0.019666	2.274998
99.148303	1633.195834	5.247206	-0.019726	2.280013
99.233625	1641.246345	5.252211	-0.019748	2.285008
99.747557	1649.302494	5.257216	-0.019849	2.290032
100.175229	1657.355897	5.262221	-0.019934	2.295036
100.352870	1665.437428	5.267226	-0.019973	2.300025
100.657880	1673.498554	5.272230	-0.020035	2.305002
100.645179	1681.598168	5.277235	-0.020039	2.309965
101.004277	1689.681196	5.282240	-0.020111	2.314938
101.209882	1697.726010	5.287245	-0.020155	2.319864
101.427746	1705.793848	5.292250	-0.020201	2.324795
101.523926	1713.889383	5.297254	-0.020225	2.329722
101.812370	1721.960513	5.302259	-0.020284	2.334639
102.215456	1730.009534	5.307264	-0.020365	2.339543
102.288804	1738.079049	5.312269	-0.020384	2.344421
102.563382	1746.170854	5.317274	-0.020441	2.349319
103.056373	1754.252278	5.322278	-0.020538	2.354218
103.280415	1762.287724	5.327283	-0.020585	2.359058
103.709948	1770.325686	5.332288	-0.020671	2.363905
103.897916	1778.379511	5.337293	-0.020712	2.368733
104.315334	1786.458090	5.342298	-0.020795	2.373584
104.597745	1794.508861	5.347302	-0.020853	2.378398
104.413089	1802.616673	5.352307	-0.020824	2.383198
104.833236	1810.675294	5.357312	-0.020908	2.388008
104.997397	1818.749545	5.362317	-0.020944	2.392797
105.275349	1826.805577	5.367322	-0.021002	2.397575
105.641575	1834.835603	5.372326	-0.021075	2.402334
105.942311	1842.875376	5.377331	-0.021137	2.407085
106.323852	1850.964971	5.382336	-0.021214	2.411862
106.526235	1859.031944	5.387341	-0.021257	2.416602
107.064648	1867.066355	5.392346	-0.021363	2.421340
107.296581	1875.145102	5.397350	-0.021412	2.426070
107.480865	1883.252250	5.402355	-0.021452	2.430804
107.846147	1891.379958	5.407360	-0.021525	2.435555
107.804328	1899.423033	5.412365	-0.021523	2.440217
108.244619	1907.437755	5.417370	-0.021611	2.444889
108.582094	1915.474849	5.422374	-0.021679	2.449558
108.868561	1923.526878	5.427379	-0.021738	2.454223
109.260079	1931.580120	5.432384	-0.021816	2.458887
109.485534	1939.619764	5.437389	-0.021864	2.463522
109.779526	1947.696279	5.442394	-0.021924	2.468175
110.109900	1955.771203	5.447398	-0.021991	2.472820
110.211743	1963.832195	5.452403	-0.022016	2.477432
110.684650	1971.850732	5.457408	-0.022110	2.482038
110.903320	1979.901547	5.462413	-0.022156	2.486636
110.998589	1988.002935	5.467418	-0.022179	2.491244
111.338972	1996.062599	5.472422	-0.022248	2.495839
111.535765	2004.117513	5.477427	-0.022290	2.500411
111.678627	2012.191775	5.482432	-0.022323	2.504983
111.837558	2020.248056	5.487437	-0.022358	2.509537
112.548042	2028.297281	5.492442	-0.022496	2.514118
112.560486	2036.379809	5.497446	-0.022504	2.518660
112.885980	2044.389435	5.502451	-0.022570	2.523174
113.222563	2052.445695	5.507456	-0.022638	2.527708
113.302503	2060.517849	5.512461	-0.022659	2.532224
113.517966	2068.583253	5.517466	-0.022704	2.536738
113.816466	2076.632940	5.522470	-0.022766	2.541241
114.040455	2084.679873	5.527475	-0.022813	2.545729
114.392030	2092.745503	5.532480	-0.022884	2.550228
114.399419	2100.823846	5.537485	-0.022891	2.554702
114.853104	2108.847684	5.542490	-0.022981	2.559170
115.111185	2116.884805	5.547494	-0.023035	2.563623
115.024372	2124.972247	5.552499	-0.023024	2.568073
115.332332	2133.028729	5.557504	-0.023087	2.572525
115.700343	2141.054240	5.562509	-0.023161	2.576956
115.956429	2149.099885	5.567514	-0.023214	2.581383
116.013069	2157.178824	5.572518	-0.023230	2.585807
116.356714	2165.227100	5.577523	-0.023300	2.590226
116.691076	2173.487370	5.582528	-0.023368	2.594753
116.902442	2181.428291	5.587533	-0.023413	2.599089
117.284004	2189.429242	5.592538	-0.023490	2.603462
117.667732	2197.440160	5.597542	-0.023567	2.607834
117.721583	2205.507500	5.602547	-0.023582	2.612206
117.774532	2213.585620	5.607552	-0.023598	2.616577
118.096752	2221.572420	5.612557	-0.023663	2.620909
118.088329	2229.639934	5.617562	-0.023667	2.625256
118.369099	2237.691776	5.622566	-0.023725	2.629606
118.541356	2245.754512	5.627571	-0.023763	2.633947
118.895235	2253.779448	5.632576	-0.023834	2.638273
118.961828	2261.810193	5.637581	-0.023852	2.642576
119.279890	2269.851273	5.642586	-0.023917	2.646894
119.623213	2277.912833	5.647590	-0.023987	2.651218
119.693981	2285.982109	5.652595	-0.024005	2.655520
119.893689	2294.035256	5.657600	-0.024048	2.659816
120.212300	2302.035256	5.662605	-0.024113	2.664084
120.328757	2310.112395	5.667610	-0.024140	2.668373
120.427587	2318.210654	5.672614	-0.024164	2.672665
120.801069	2326.237211	5.677619	-0.024239	2.676930
121.090184	2334.251482	5.682624	-0.024299	2.681176
121.206042	2342.304940	5.687629	-0.024326	2.685426
121.524542	2350.321793	5.692634	-0.024391	2.689661
121.625941	2358.415752	5.697638	-0.024415	2.693917
121.601201	2366.463260	5.702643	-0.024416	2.698134
121.762967	2374.514662	5.707648	-0.024452	2.702358
122.022009	2382.538986	5.712653	-0.024506	2.706568
122.134373	2390.595334	5.717658	-0.024532	2.710778
122.436631	2398.660756	5.722662	-0.024594	2.714998
122.743338	2406.659685	5.727667	-0.024657	2.719178
123.029594	2414.704830	5.732672	-0.024716	2.723373
123.130124	2422.755140	5.737677	-0.024740	2.727554
123.448103	2430.816162	5.742682	-0.024805	2.731747
123.825933	2438.857877	5.747686	-0.024881	2.735927
123.883896	2446.907028	5.752691	-0.024897	2.740085
124.064084	2454.960660	5.757696	-0.024936	2.744246
124.267789	2462.990455	5.762701	-0.024980	2.748390
124.431320	2471.113856	5.767706	-0.025016	2.752574
124.654774	2479.175060	5.772710	-0.025063	2.756722
125.036015	2487.155588	5.777715	-0.025140	2.760833
125.417414	2495.169597	5.782720	-0.025216	2.764955
125.429563	2503.209050	5.787725	-0.025224	2.769061
125.668746	2511.274962	5.792730	-0.025274	2.773188
125.593907	2519.354708	5.797734	-0.025266	2.777298
125.843318	2527.361289	5.802739	-0.025318	2.781383
126.123432	2535.402067	5.807744	-0.025376	2.785482
126.256405	2543.431263	5.812749	-0.025406	2.789560
126.569229	2551.490327	5.817754	-0.025470	2.793658
126.690536	2559.547721	5.822758	-0.025498	2.797737
127.093047	2567.547936	5.827763	-0.025579	2.801798
127.453357	2575.572919	5.832768	-0.025651	2.805863
127.516097	2583.622906	5.837773	-0.025669	2.809918
127.945590	2591.672248	5.842778	-0.025754	2.813987
128.407250	2599.696799	5.847782	-0.025846	2.818040
128.655553	2607.717077	5.852787	-0.025897	2.822073
128.916469	2615.789996	5.857792	-0.025952	2.826127
129.299777	2623.816285	5.862797	-0.026029	2.830159
129.543162	2631.912775	5.867802	-0.026080	2.834212
129.683881	2639.940487	5.872806	-0.026111	2.838219
129.913389	2647.956355	5.877811	-0.026160	2.842219
130.288371	2655.988540	5.882816	-0.026235	2.846231
130.407493	2664.022814	5.887821	-0.026263	2.850223
130.527810	2672.101088	5.892826	-0.026291	2.854231
130.862364	2680.134414	5.897830	-0.026359	2.858223
130.998031	2688.161082	5.902835	-0.026389	2.862196
131.387361	2696.184402	5.907840	-0.026468	2.866175
131.749142	2704.215843	5.912845	-0.026540	2.870151
131.904782	2712.299505	5.917850	-0.026575	2.874136
132.167527	2720.325260	5.922854	-0.026630	2.878093
132.160825	2728.372547	5.927859	-0.026634	2.882040
132.580445	2736.420990	5.932864	-0.026718	2.886006
132.711992	2744.445728	5.937869	-0.026748	2.889939
132.962540	2752.509192	5.942874	-0.026800	2.893891
133.158045	2760.557907	5.947878	-0.026842	2.897828
133.265515	2768.594079	5.952883	-0.026868	2.901749
133.349358	2776.663060	5.957888	-0.026889	2.905680
133.551174	2784.667640	5.962893	-0.026932	2.909580
133.843110	2792.803864	5.967898	-0.026992	2.913543
134.096072	2800.798940	5.972902	-0.027045	2.917431
134.464370	2808.779906	5.977907	-0.027119	2.921312
134.725715	2816.797626	5.982912	-0.027173	2.925201
134.837601	2824.833435	5.987917	-0.027199	2.929085
135.016570	2832.879790	5.992922	-0.027238	2.932972
135.329923	2840.926183	5.997926	-0.027302	2.936862
135.516435	2848.958213	6.002931	-0.027342	2.940732
135.739356	2856.965744	6.007936	-0.027390	2.944588
135.658777	2865.046097	6.012941	-0.027380	2.948458
136.036984	2873.081551	6.017946	-0.027456	2.952325
136.254907	2881.139824	6.022950	-0.027502	2.956189
136.246837	2889.155261	6.027955	-0.027506	2.960016
136.419769	2897.204845	6.032960	-0.027544	2.963864
136.689959	2905.195516	6.037965	-0.027600	2.967684
136.834747	2913.250790	6.042970	-0.027633	2.971523
136.917366	2921.354782	6.047974	-0.027654	2.975377
137.046944	2929.324726	6.052979	-0.027683	2.979165
137.324044	2937.369602	6.057984	-0.027740	2.982991
137.406253	2945.411365	6.062989	-0.027761	2.986801
137.780198	2953.440403	6.067994	-0.027837	2.990614
137.875785	2961.533223	6.072998	-0.027860	2.994439
138.096531	2969.511212	6.078003	-0.027907	2.998211
138.593041	2977.522672	6.083008	-0.028005	3.002008
138.671287	2985.558730	6.088013	-0.028025	3.005790
138.967416	2993.578711	6.093018	-0.028086	3.009572
139.155970	3001.700831	6.098022	-0.028126	3.013390
139.280887	3009.692645	6.103027	-0.028155	3.017140
139.654395	3017.711871	6.108032	-0.028230	3.020910
139.777023	3025.736091	6.113037	-0.028259	3.024666
139.917667	3033.796594	6.118042	-0.028290	3.028434
140.133064	3041.865474	6.123046	-0.028336	3.032206
140.145478	3049.900503	6.128051	-0.028344	3.035947
140.547091	3057.906463	6.133056	-0.028424	3.039689
140.793300	3065.910998	6.138061	-0.028476	3.043417
140.868549	3073.961324	6.143066	-0.028495	3.047155
141.230218	3081.994759	6.148070	-0.028568	3.050893
141.243461	3090.032221	6.153075	-0.028576	3.054613
141.539228	3098.080909	6.158080	-0.028637	3.058346
141.600081	3106.138621	6.163085	-0.028654	3.062068
142.077016	3114.129056	6.168090	-0.028748	3.065774
142.252493	3122.188684	6.173094	-0.028787	3.069492
142.383905	3130.285774	6.178099	-0.028817	3.073222
143.057577	3138.294780	6.183104	-0.028948	3.076932
143.354695	3146.286648	6.188109	-0.029009	3.080612
143.556221	3154.291779	6.193114	-0.029052	3.084289
143.777853	3162.334578	6.198118	-0.029098	3.087980
144.012824	3170.365271	6.203123	-0.029148	3.091661
144.189725	3178.455991	6.208128	-0.029186	3.095363
144.318116	3186.450384	6.213133	-0.029216	3.099014
144.477265	3194.482059	6.218138	-0.029251	3.102679
144.634613	3202.526934	6.223142	-0.029286	3.106346
144.695718	3210.553894	6.228147	-0.029303	3.109996
144.908889	3218.615079	6.233152	-0.029348	3.113664
145.253986	3226.607973	6.238157	-0.029418	3.117303
145.356610	3234.647587	6.243162	-0.029443	3.120947
145.832760	3242.634062	6.248166	-0.029537	3.124580
146.011726	3250.666408	6.253171	-0.029576	3.128217
146.219994	3258.758618	6.258176	-0.029620	3.131877
146.130897	3266.825253	6.263181	-0.029609	3.135508
146.403608	3274.806617	6.268186	-0.029665	3.139113
146.652666	3282.846869	6.273190	-0.029717	3.142739
146.876098	3290.843401	6.278195	-0.029765	3.146340
147.101497	3298.910307	6.283200	-0.029812	3.149968
147.176484	3306.975519	6.288205	-0.029832	3.153585
147.367435	3315.008027	6.293210	-0.029873	3.157188
147.551678	3323.029502	6.298214	-0.029913	3.160782
147.749481	3331.009217	6.303219	-0.029955	3.164353
148.209781	3339.040580	6.308224	-0.030046	3.167955
148.091216	3347.120425	6.313229	-0.030030	3.171549
148.236815	3355.131261	6.318234	-0.030063	3.175120
148.697476	3363.153204	6.323238	-0.030154	3.178706
148.965958	3371.167718	6.328243	-0.030210	3.182275
149.139437	3379.229360	6.333248	-0.030247	3.185858
149.338035	3387.247698	6.338253	-0.030290	3.189418
149.596499	3395.299040	6.343258	-0.030344	3.192992
149.686887	3403.372722	6.348262	-0.030366	3.196564
149.869767	3411.349758	6.353267	-0.030406	3.200093
150.165517	3419.376700	6.358272	-0.030466	3.203646
150.150027	3427.423736	6.363277	-0.030469	3.207190
150.280147	3435.459526	6.368282	-0.030499	3.210731
150.521434	3443.507992	6.373286	-0.030549	3.214278
150.589147	3451.536985	6.378291	-0.030568	3.217806
150.879714	3459.566726	6.383296	-0.030627	3.221340
151.039339	3467.552102	6.388301	-0.030663	3.224845
151.220979	3475.621288	6.393306	-0.030702	3.228383
151.481985	3483.694877	6.398310	-0.030756	3.231923
151.711776	3491.719551	6.403315	-0.030805	3.235436
152.136378	3499.684114	6.408320	-0.030889	3.238927
152.108246	3507.701618	6.413325	-0.030889	3.242419
152.388136	3515.716482	6.418330	-0.030947	3.245918
152.527643	3523.757415	6.423334	-0.030979	3.249420
152.759976	3531.797104	6.428339	-0.031028	3.252920
152.968997	3539.842679	6.433344	-0.031072	3.256419
153.118942	3547.813050	6.438349	-0.031106	3.259879
153.218397	3555.882466	6.443354	-0.031130	3.263376
153.364069	3563.943368	6.448358	-0.031162	3.266867
153.558140	3571.952875	6.453363	-0.031204	3.270334
153.887341	3579.999955	6.458368	-0.031271	3.273819
154.058228	3588.027392	6.463373	-0.031308	3.277286
154.117358	3596.038719	6.468378	-0.031325	3.280738
154.475957	3604.032176	6.473382	-0.031397	3.284190
154.578120	3612.065353	6.478387	-0.031422	3.287645
154.924789	3620.140344	6.483392	-0.031492	3.291124
155.125930	3628.169369	6.488397	-0.031535	3.294574
155.356927	3636.178713	6.493402	-0.031584	3.298014
155.467781	3644.247436	6.498406	-0.031610	3.301470
155.693441	3652.209918	6.503411	-0.031657	3.304882
155.826829	3660.277486	6.508416	-0.031688	3.308331
155.863276	3668.332131	6.513421	-0.031700	3.311768
156.077641	3676.404324	6.518426	-0.031746	3.315215
156.350222	3684.377866	6.523430	-0.031802	3.318619
156.534567	3692.377806	6.528435	-0.031842	3.322028
156.616177	3700.433347	6.533440	-0.031863	3.325452
156.824389	3708.425747	6.538445	-0.031907	3.328851
156.906527	3716.476534	6.543450	-0.031928	3.332266
157.091189	3724.542890	6.548454	-0.031968	3.335689
157.115298	3732.522346	6.553459	-0.031978	3.339065
157.455158	3740.548190	6.558464	-0.032047	3.342469
157.671041	3748.560600	6.563469	-0.032093	3.345859
157.887815	3756.580429	6.568474	-0.032139	3.349249
158.263466	3764.631084	6.573478	-0.032214	3.352654
158.404858	3772.657631	6.578483	-0.032246	3.356037
158.564051	3780.695276	6.583488	-0.032281	3.359422
158.744752	3788.718439	6.588493	-0.032320	3.362798
159.179323	3796.731720	6.593498	-0.032407	3.366176
159.339445	3804.796113	6.598502	-0.032442	3.369562
159.408041	3812.834734	6.603507	-0.032461	3.372930
159.774125	3820.864320	6.608512	-0.032534	3.376302
159.883774	3828.876803	6.613517	-0.032560	3.379654
159.853847	3836.909128	6.618522	-0.032560	3.383006
160.302358	3844.951655	6.623526	-0.032649	3.386376
160.441771	3852.925773	6.628531	-0.032681	3.389703
160.664444	3861.075655	6.633536	-0.032728	3.393103
161.148418	3869.079668	6.638541	-0.032824	3.396448
161.535245	3877.013466	6.643546	-0.032901	3.399757
161.704799	3885.055388	6.648550	-0.032938	3.403100
161.724812	3893.063525	6.653555	-0.032948	3.406420
161.996089	3901.088005	6.658560	-0.033004	3.409753
161.981111	3909.138189	6.663565	-0.033007	3.413083
162.235951	3917.184476	6.668570	-0.033060	3.416418
162.628975	3925.170607	6.673574	-0.033138	3.419729
162.733897	3933.197496	6.678579	-0.033164	3.423044
162.823820	3941.235731	6.683584	-0.033186	3.426360
162.750797	3949.283028	6.688589	-0.033178	3.429671
163.150789	3957.295576	6.693594	-0.033258	3.432980
163.368488	3965.335491	6.698598	-0.033304	3.436291
163.250492	3973.339088	6.703603	-0.033288	3.439573
163.456177	3981.379581	6.708608	-0.033332	3.442878
163.725869	3989.389174	6.713613	-0.033387	3.446169
164.155883	3997.405805	6.718618	-0.033473	3.449465
164.294590	4005.480538	6.723622	-0.033504	3.452771
164.590353	4013.477821	6.728627	-0.033565	3.456049
164.626543	4021.519744	6.733632	-0.033577	3.459332
164.688476	4029.523611	6.738637	-0.033594	3.462598
165.287068	4037.531308	6.743642	-0.033711	3.465880
165.635696	4045.574474	6.748646	-0.033782	3.469165
165.475649	4053.675849	6.753651	-0.033758	3.472454
165.831564	4061.691646	6.758656	-0.033830	3.475722
165.908360	4069.677975	6.763661	-0.033849	3.478966
165.817352	4077.706610	6.768666	-0.033838	3.482218
166.274574	4085.700339	6.773670	-0.033929	3.485471
166.335986	4093.722025	6.778675	-0.033946	3.488719
166.635069	4101.777417	6.783680	-0.034007	3.491986
166.661577	4109.793747	6.788685	-0.034018	3.495225
166.954086	4117.796030	6.793690	-0.034078	3.498464
167.261390	4125.841907	6.798694	-0.034140	3.501718
167.398181	4133.827996	6.803699	-0.034171	3.504939
167.625629	4141.863386	6.808704	-0.034219	3.508180
167.750100	4149.937570	6.813709	-0.034248	3.511430
167.780238	4157.953468	6.818714	-0.034259	3.514651
168.230938	4165.965474	6.823718	-0.034349	3.517880
168.527658	4173.999963	6.828723	-0.034410	3.521111
168.678087	4181.974395	6.833728	-0.034443	3.524310
168.709600	4190.027641	6.838733	-0.034455	3.527534
169.048929	4198.036770	6.843738	-0.034523	3.530747
169.360358	4206.112548	6.848742	-0.034587	3.533983
169.343250	4214.135410	6.853747	-0.034589	3.537184
169.268798	4222.175347	6.858752	-0.034581	3.540388
169.474192	4230.179545	6.863757	-0.034625	3.543583
169.629015	4238.230958	6.868762	-0.034659	3.546793
169.736275	4246.263454	6.873766	-0.034685	3.549990
170.141224	4254.311698	6.878771	-0.034766	3.553200
170.297009	4262.402478	6.883776	-0.034800	3.556416
170.351999	4270.331730	6.888781	-0.034816	3.559563
170.510923	4278.367538	6.893786	-0.034851	3.562751
170.876456	4286.374858	6.898790	-0.034925	3.565932
170.889916	4294.361730	6.903795	-0.034933	3.569092
171.117106	4302.422195	6.908800	-0.034981	3.572284
171.432466	4310.430519	6.913805	-0.035045	3.575455
171.565295	4318.444394	6.918810	-0.035076	3.578620
171.765730	4326.484282	6.923814	-0.035118	3.581794
171.753106	4334.468356	6.928819	-0.035122	3.584938
171.969119	4342.500030	6.933824	-0.035167	3.588104
172.127029	4350.563764	6.938829	-0.035202	3.591278
172.299170	4358.581195	6.943834	-0.035240	3.594431
172.679609	4366.592370	6.948838	-0.035317	3.597585
172.545550	4374.600636	6.953843	-0.035297	3.600721
172.633135	4382.629487	6.958848	-0.035319	3.603869
172.943070	4390.638375	6.963853	-0.035382	3.607011
173.216548	4398.651397	6.968858	-0.035439	3.610152
173.424483	4406.726547	6.973862	-0.035483	3.613313
173.596858	4414.703353	6.978867	-0.035521	3.616431
174.068034	4422.726124	6.983872	-0.035614	3.619572
174.167293	4430.742964	6.988877	-0.035638	3.622699
174.134020	4438.788112	6.993882	-0.035637	3.625830
174.443493	4446.835507	6.998886	-0.035701	3.628968
174.634251	4454.866952	7.003891	-0.035742	3.632095
174.949566	4462.921684	7.008896	-0.035806	3.635231
175.127523	4470.916563	7.013901	-0.035845	3.638337
175.216732	4478.926917	7.018906	-0.035867	3.641445
175.340510	4486.925647	7.023910	-0.035896	3.644546
175.360350	4494.972303	7.028915	-0.035905	3.647660
175.428306	4503.029015	7.033920	-0.035923	3.650777
175.559513	4511.057600	7.038925	-0.035953	3.653881
175.789532	4519.069349	7.043930	-0.036002	3.656980
175.963567	4527.084519	7.048934	-0.036039	3.660075
176.207997	4535.073416	7.053939	-0.036091	3.663160
176.236946	4543.167296	7.058944	-0.036102	3.666276
176.398804	4551.121084	7.063949	-0.036137	3.669340
176.488397	4559.182354	7.068954	-0.036160	3.672440
176.699137	4567.249685	7.073958	-0.036204	3.675544
176.965565	4575.173682	7.078963	-0.036259	3.678591
177.224062	4583.241782	7.083968	-0.036313	3.681690
177.282931	4591.215089	7.088973	-0.036330	3.684746
177.302673	4599.259665	7.093978	-0.036339	3.687825
177.641741	4607.309494	7.098982	-0.036408	3.690912
177.744462	4615.332735	7.103987	-0.036432	3.693980
177.817805	4623.373629	7.108992	-0.036452	3.697051
177.812350	4631.364176	7.113997	-0.036456	3.700099
178.281457	4639.368039	7.119002	-0.036549	3.703161
178.393606	4647.429860	7.124006	-0.036576	3.706234
178.395710	4655.401315	7.129011	-0.036581	3.709267
178.730764	4663.523723	7.134016	-0.036650	3.712363
178.655176	4671.589103	7.139021	-0.036641	3.715425
178.763270	4679.514339	7.144026	-0.036667	3.718435
179.114022	4687.560627	7.149030	-0.036738	3.721495
179.274704	4695.479948	7.154035	-0.036773	3.724500
179.428825	4703.537329	7.159040	-0.036807	3.727554
179.569346	4711.569232	7.164045	-0.036839	3.730596
179.736713	4719.606887	7.169050	-0.036876	3.733638
179.725957	4727.689715	7.174054	-0.036879	3.736690
179.897024	4735.643562	7.179059	-0.036917	3.739696
180.287787	4743.680395	7.184064	-0.036995	3.742735
180.406459	4751.693705	7.189069	-0.037023	3.745757
180.342648	4759.709991	7.194074	-0.037016	3.748773
180.687644	4767.787847	7.199078	-0.037086	3.751820
180.962994	4775.786160	7.204083	-0.037143	3.754832
181.090530	4783.774373	7.209088	-0.037172	3.757835
181.175482	4791.833256	7.214093	-0.037194	3.760861
181.373992	4799.794238	7.219098	-0.037236	3.763850
181.707051	4807.824277	7.224102	-0.037304	3.766866
181.856402	4815.874613	7.229107	-0.037337	3.769883
182.251048	4823.924910	7.234112	-0.037416	3.772902
182.387523	4831.979096	7.239117	-0.037447	3.775916
182.159557	4839.990702	7.244122	-0.037411	3.778902
182.395990	4847.996497	7.249126	-0.037460	3.781894
182.515990	4855.993113	7.254131	-0.037488	3.784878
182.663780	4864.017913	7.259136	-0.037521	3.787871
182.696974	4872.062677	7.264141	-0.037533	3.790866
182.925180	4880.117351	7.269146	-0.037581	3.793867
183.272300	4888.126925	7.274150	-0.037651	3.796852
183.272828	4896.096139	7.279155	-0.037657	3.799811
183.758660	4904.089307	7.284160	-0.037753	3.802788
183.848870	4912.128169	7.289165	-0.037775	3.805770
184.022877	4920.154995	7.294170	-0.037813	3.808747
184.180612	4928.205166	7.299174	-0.037848	3.811731
184.407230	4936.178348	7.304179	-0.037896	3.814685
184.508342	4944.223387	7.309184	-0.037920	3.817660
184.439147	4952.228763	7.314189	-0.037913	3.820615
184.831820	4960.221379	7.319194	-0.037992	3.823573
184.929884	4968.317709	7.324198	-0.038016	3.826561
184.849026	4976.283135	7.329203	-0.038006	3.829494
185.137047	4984.370234	7.334208	-0.038065	3.832477
185.244971	4992.362760	7.339213	-0.038091	3.835420
185.308715	5000.346982	7.344218	-0.038108	3.838356
185.533894	5008.405640	7.349222	-0.038156	3.841321
185.775815	5016.348000	7.354227	-0.038206	3.844241
185.714060	5024.413136	7.359232	-0.038201	3.847197
185.830238	5032.472835	7.364237	-0.038228	3.850153
186.071011	5040.496043	7.369242	-0.038278	3.853096
186.454677	5048.521002	7.374246	-0.038355	3.856040
186.572545	5056.524215	7.379251	-0.038383	3.858968
186.883923	5064.569951	7.384256	-0.038446	3.861914
187.014705	5072.562561	7.389261	-0.038476	3.864834
187.094169	5080.624872	7.394266	-0.038497	3.867777
187.259516	5088.667274	7.399270	-0.038533	3.870711
187.230243	5096.872182	7.404275	-0.038533	3.873699
187.632654	5104.867026	7.409280	-0.038614	3.876617
187.805848	5112.725813	7.414285	-0.038651	3.879478
188.027908	5120.717643	7.419290	-0.038698	3.882386
188.170648	5128.762810	7.424294	-0.038730	3.885311
188.025486	5136.754538	7.429299	-0.038709	3.888207
188.128280	5144.790712	7.434304	-0.038734	3.891123
188.207239	5152.829053	7.439309	-0.038754	3.894037
188.541318	5160.822072	7.444314	-0.038822	3.896937
188.516158	5168.817583	7.449318	-0.038823	3.899829
188.639595	5176.838911	7.454323	-0.038851	3.902731
188.714132	5184.864493	7.459328	-0.038871	3.905631
188.916730	5192.896363	7.464333	-0.038914	3.908534
189.179044	5200.899174	7.469338	-0.038968	3.911425
189.424327	5208.962633	7.474342	-0.039020	3.914336
189.630762	5216.950075	7.479347	-0.039064	3.917216
189.718179	5224.955645	7.484352	-0.039085	3.920099
189.780417	5232.965828	7.489357	-0.039103	3.922980
189.773816	5240.961957	7.494362	-0.039107	3.925853
190.126282	5249.004968	7.499366	-0.039178	3.928748
190.221660	5257.030439	7.504371	-0.039201	3.931629
190.637776	5265.057974	7.509376	-0.039285	3.934515
190.572769	5273.072008	7.514381	-0.039278	3.937385
190.733669	5281.071046	7.519386	-0.039313	3.940252
190.974889	5289.116532	7.524390	-0.039364	3.943134
190.984572	5297.127015	7.529395	-0.039371	3.945998
190.892787	5305.137822	7.534400	-0.039360	3.948858
191.159605	5313.193731	7.539405	-0.039415	3.951738
191.479880	5321.201376	7.544410	-0.039480	3.954600
191.506441	5329.236231	7.549414	-0.039491	3.957465
191.851667	5337.210666	7.554419	-0.039561	3.960311
191.977312	5345.237540	7.559424	-0.039590	3.963170
191.911425	5353.282091	7.564429	-0.039583	3.966030
192.151894	5361.250134	7.569434	-0.039633	3.968866
192.277859	5369.316491	7.574438	-0.039662	3.971733
192.358986	5377.311660	7.579443	-0.039683	3.974572
192.645996	5385.361878	7.584448	-0.039742	3.977432
192.654159	5393.380006	7.589453	-0.039749	3.980273
192.952779	5401.377057	7.594458	-0.039810	3.983110
193.056360	5409.416390	7.599462	-0.039835	3.985957
193.101295	5417.426266	7.604467	-0.039849	3.988790
193.275271	5425.484511	7.609472	-0.039887	3.991641
193.496663	5433.528728	7.614477	-0.039934	3.994485
193.498290	5441.524237	7.619482	-0.039940	3.997306
193.795462	5449.564178	7.624486	-0.040001	4.000146
193.955960	5457.543493	7.629491	-0.040036	4.002960
194.098611	5465.562124	7.634496	-0.040068	4.005786
194.371921	5473.608117	7.639501	-0.040125	4.008621
194.624661	5481.640423	7.644506	-0.040177	4.011449
194.752949	5489.698291	7.649510	-0.040207	4.014283
194.594635	5497.693707	7.654515	-0.040183	4.017087
195.065726	5505.684602	7.659520	-0.040276	4.019898
195.193891	5513.717783	7.664525	-0.040306	4.022717
195.115567	5521.711343	7.669530	-0.040297	4.025517
195.476579	5529.752805	7.674534	-0.040369	4.028338
195.395785	5537.771070	7.679539	-0.040360	4.031142
195.579110	5545.897798	7.684544	-0.040400	4.033986
195.809461	5553.889767	7.689549	-0.040448	4.036782
196.127663	5561.812053	7.694554	-0.040513	4.039552
196.373184	5569.848647	7.699558	-0.040564	4.042360
196.327833	5577.815517	7.704563	-0.040561	4.045137
196.648831	5585.874539	7.709568	-0.040627	4.047950
196.768842	5593.886776	7.714573	-0.040655	4.050741
196.832037	5601.904287	7.719578	-0.040672	4.053532
197.391427	5609.937195	7.724582	-0.040782	4.056333
197.457686	5617.887611	7.729587	-0.040799	4.059096
197.558198	5625.954503	7.734592	-0.040824	4.061898
197.872119	5633.924623	7.739597	-0.040888	4.064668
197.910287	5641.959348	7.744602	-0.040900	4.067454
197.957219	5649.997446	7.749606	-0.040915	4.070240
197.968437	5658.037116	7.754611	-0.040922	4.073024
198.270372	5666.056124	7.759616	-0.040984	4.075803
198.309664	5674.061482	7.764621	-0.040997	4.078572
198.479829	5682.070688	7.769626	-0.041034	4.081341
198.761206	5690.050238	7.774630	-0.041092	4.084101
199.010089	5698.069179	7.779635	-0.041144	4.086871
199.225609	5706.099515	7.784640	-0.041190	4.089643
199.417074	5714.153560	7.789645	-0.041231	4.092421
199.376461	5722.188659	7.794650	-0.041229	4.095187
199.881744	5730.186220	7.799654	-0.041329	4.097946
199.972135	5738.188151	7.804659	-0.041351	4.100699
199.998014	5746.193439	7.809664	-0.041362	4.103451
200.220096	5754.227540	7.814669	-0.041409	4.106213
200.191929	5762.254825	7.819674	-0.041409	4.108967
200.542426	5770.321432	7.824678	-0.041480	4.111738
200.533956	5778.342446	7.829683	-0.041484	4.114487
200.789958	5786.356192	7.834688	-0.041537	4.117235
200.764114	5794.348492	7.839693	-0.041538	4.119971
201.060617	5802.362463	7.844698	-0.041599	4.122715
201.168008	5810.365119	7.849702	-0.041624	4.125452
201.003433	5818.383113	7.854707	-0.041599	4.128189
201.233055	5826.418524	7.859712	-0.041647	4.130935
201.457283	5834.483383	7.864717	-0.041695	4.133689
201.472672	5842.491631	7.869722	-0.041703	4.136419
201.609636	5850.525574	7.874726	-0.041734	4.139157
201.813699	5858.498293	7.879731	-0.041778	4.141874
201.995628	5866.469781	7.884736	-0.041817	4.144588
202.184758	5874.599722	7.889741	-0.041858	4.147355
202.448043	5882.545983	7.894746	-0.041913	4.150058
202.663050	5890.625236	7.899750	-0.041958	4.152804
202.602247	5898.635752	7.904755	-0.041952	4.155521
202.882211	5906.629600	7.909760	-0.042010	4.158235
203.236424	5914.629932	7.914765	-0.042082	4.160950
203.082162	5922.628098	7.919770	-0.042058	4.163657
203.077816	5930.683541	7.924774	-0.042063	4.166383
203.546528	5938.665511	7.929779	-0.042156	4.169088
203.665277	5946.716351	7.934784	-0.042184	4.171810
203.524230	5954.756208	7.939789	-0.042163	4.174524
203.969874	5962.734605	7.944794	-0.042252	4.177222
204.063673	5970.773465	7.949798	-0.042275	4.179935
204.021125	5978.755358	7.954803	-0.042272	4.182625
204.329284	5986.769891	7.959808	-0.042335	4.185329
204.733294	5994.839514	7.964813	-0.042416	4.188050
204.759708	6002.796756	7.969818	-0.042427	4.190727
205.025163	6010.976243	7.974822	-0.042482	4.193480
205.285623	6018.966192	7.979827	-0.042536	4.196168
205.353683	6026.873521	7.984832	-0.042554	4.198824
205.527303	6034.943581	7.989837	-0.042592	4.201533
205.325089	6042.862102	7.994842	-0.042560	4.204187
205.581223	6050.935340	7.999846	-0.042613	4.206895
205.587542	6058.937673	8.004851	-0.042620	4.209575
205.750070	6066.950595	8.009856	-0.042656	4.212259
205.877219	6074.996855	8.014861	-0.042685	4.214952
206.165906	6083.006066	8.019866	-0.042744	4.217632
206.368487	6091.020280	8.024870	-0.042787	4.220311
206.554508	6098.990593	8.029875	-0.042828	4.222974
206.878557	6107.016218	8.034880	-0.042893	4.225655
206.699673	6115.058150	8.039885	-0.042866	4.228335
206.817880	6123.069244	8.044890	-0.042893	4.231005
207.156737	6131.145628	8.049894	-0.042962	4.233698
207.254148	6139.140428	8.054899	-0.042986	4.236359
207.403661	6147.106883	8.059904	-0.043019	4.239010
207.697932	6155.174809	8.064909	-0.043079	4.241695
207.547868	6163.148659	8.069914	-0.043057	4.244342
207.751088	6171.197476	8.074918	-0.043101	4.247015
207.972024	6179.170001	8.079923	-0.043147	4.249662
208.040155	6187.236608	8.084928	-0.043165	4.252337
208.206126	6195.291500	8.089933	-0.043202	4.255007
208.063308	6203.260929	8.094938	-0.043181	4.257645
208.360350	6211.293157	8.099942	-0.043242	4.260306
208.332146	6219.271300	8.104947	-0.043242	4.262944
208.372929	6227.299785	8.109952	-0.043255	4.265597
208.848709	6235.313238	8.114957	-0.043349	4.268248
209.091664	6243.356931	8.119962	-0.043400	4.270905
209.191428	6251.465344	8.124966	-0.043424	4.273581
209.206619	6259.462666	8.129971	-0.043433	4.276217
209.416292	6267.434333	8.134976	-0.043477	4.278846
209.540450	6275.504238	8.139981	-0.043506	4.281504
209.543448	6283.400063	8.144986	-0.043512	4.284102
209.793189	6291.511004	8.149990	-0.043564	4.286771
209.887567	6299.458993	8.154995	-0.043587	4.289384
209.907697	6307.557294	8.160000	-0.043597	4.292044
210.130421	6315.565264	8.165005	-0.043644	4.294674
210.272145	6323.616396	8.170010	-0.043676	4.297316
210.560449	6331.585170	8.175014	-0.043735	4.299931
210.631657	6339.581288	8.180019	-0.043754	4.302551
210.646357	6347.569357	8.185024	-0.043762	4.305167
210.777835	6355.613939	8.190029	-0.043792	4.307800
210.834919	6363.603175	8.195034	-0.043808	4.310413
211.103360	6371.715646	8.200038	-0.043864	4.313067
211.328527	6379.729051	8.205043	-0.043912	4.315686
211.405766	6387.708705	8.210048	-0.043931	4.318291
211.618053	6395.704519	8.215053	-0.043977	4.320901
211.791760	6403.652485	8.220058	-0.044014	4.323494
211.974309	6411.753667	8.225062	-0.044054	4.326135
212.083004	6419.728200	8.230067	-0.044080	4.328732
212.210401	6427.785857	8.235072	-0.044109	4.331355
212.469785	6435.843677	8.240077	-0.044163	4.333978
212.497232	6443.812508	8.245082	-0.044174	4.336568
212.781778	6451.762384	8.250086	-0.044232	4.339152
212.832141	6459.860585	8.255091	-0.044247	4.341782
212.899449	6467.825725	8.260096	-0.044265	4.344366
212.876589	6475.886117	8.265101	-0.044267	4.346980
213.218640	6483.865815	8.270106	-0.044336	4.349568
213.439412	6491.959912	8.275110	-0.044383	4.352191
213.489564	6500.028650	8.280115	-0.044397	4.354803
213.889290	6507.990062	8.285120	-0.044477	4.357380
213.858423	6515.950360	8.290125	-0.044477	4.359954
213.898311	6523.957472	8.295130	-0.044490	4.362541
214.180095	6531.940503	8.300134	-0.044548	4.365120
214.310868	6539.976753	8.305139	-0.044578	4.367714
214.237481	6548.012028	8.310144	-0.044570	4.370305
214.616211	6556.021284	8.315149	-0.044646	4.372889
214.787401	6564.029595	8.320154	-0.044684	4.375470
214.752677	6572.089175	8.325158	-0.044683	4.378064
214.813630	6580.058610	8.330163	-0.044700	4.380628
215.108294	6588.066422	8.335168	-0.044760	4.383205
215.309220	6596.097261	8.340173	-0.044803	4.385787
215.187965	6604.103582	8.345178	-0.044786	4.388358
215.495585	6612.189797	8.350182	-0.044849	4.390955
215.669884	6620.155693	8.355187	-0.044887	4.393511
215.759065	6628.211526	8.360192	-0.044909	4.396094
215.982873	6636.201650	8.365197	-0.044956	4.398656
216.112671	6644.224423	8.370202	-0.044986	4.401225
216.309441	6652.200102	8.375206	-0.045028	4.403779
216.452225	6660.247768	8.380211	-0.045060	4.406353
216.817485	6668.250721	8.385216	-0.045134	4.408913
216.826240	6676.335488	8.390221	-0.045141	4.411496
216.815491	6684.326519	8.395226	-0.045145	4.414048
216.864564	6692.396612	8.400230	-0.045160	4.416623
217.210951	6700.305330	8.405235	-0.045230	4.419147
217.437366	6708.366516	8.410240	-0.045277	4.421717
217.622038	6716.385072	8.415245	-0.045317	4.424272
217.869012	6724.478062	8.420250	-0.045369	4.426850
217.874182	6732.441957	8.425254	-0.045375	4.429384
217.984425	6740.453118	8.430259	-0.045401	4.431931
218.228926	6748.496531	8.435264	-0.045453	4.434489
218.582823	6756.527441	8.440269	-0.045524	4.437041
218.501971	6764.450034	8.445274	-0.045514	4.439555
218.778161	6772.526824	8.450278	-0.045572	4.442119
219.115228	6780.455902	8.455283	-0.045640	4.444634
219.145293	6788.537527	8.460288	-0.045651	4.447195
219.272493	6796.531855	8.465293	-0.045680	4.449727
219.190404	6804.590684	8.470298	-0.045671	4.452278
219.644639	6812.592106	8.475302	-0.045761	4.454811
219.676529	6820.653857	8.480307	-0.045772	4.457359
219.819592	6828.607209	8.485312	-0.045804	4.459873
220.080845	6836.639848	8.490317	-0.045859	4.462411
220.105063	6844.610690	8.495322	-0.045869	4.464926
220.326650	6852.673862	8.500326	-0.045916	4.467470
220.368196	6860.671454	8.505331	-0.045929	4.469992
220.638516	6868.718611	8.510336	-0.045985	4.472528
220.475226	6876.766281	8.515341	-0.045960	4.475062
220.514928	6884.699174	8.520346	-0.045973	4.477558
220.711755	6892.718258	8.525350	-0.046015	4.480081
220.851824	6900.733597	8.530355	-0.046047	4.482601
220.917931	6908.757246	8.535360	-0.046065	4.485122
221.231659	6916.827725	8.540365	-0.046129	4.487657
221.400073	6924.805805	8.545370	-0.046166	4.490161
221.619485	6932.846670	8.550374	-0.046212	4.492684
221.538467	6940.839186	8.555379	-0.046202	4.495189
221.660208	6948.851214	8.560384	-0.046231	4.497699
221.774009	6956.893778	8.565389	-0.046257	4.500218
221.978209	6964.887212	8.570394	-0.046301	4.502720
222.121803	6972.875718	8.575399	-0.046333	4.505219
222.260955	6980.920714	8.580403	-0.046365	4.507734
222.293610	6988.936157	8.585408	-0.046376	4.510238
222.505373	6997.036649	8.590413	-0.046421	4.512768
222.689027	7005.016907	8.595418	-0.046461	4.515259
222.757516	7013.011545	8.600423	-0.046480	4.517752
222.883066	7020.968131	8.605427	-0.046508	4.520233
223.020343	7028.980183	8.610432	-0.046540	4.522729
223.358820	7037.000314	8.615437	-0.046608	4.525227
223.503583	7044.999257	8.620442	-0.046641	4.527716
223.756908	7053.044113	8.625447	-0.046693	4.530219
223.678024	7061.085635	8.630451	-0.046684	4.532718
223.806123	7069.085037	8.635456	-0.046714	4.535204
223.954082	7077.098821	8.640461	-0.046747	4.537692
224.059812	7085.067005	8.645466	-0.046772	4.540165
224.138874	7093.117264	8.650471	-0.046792	4.542662
224.338240	7101.106853	8.655475	-0.046835	4.545139
224.408375	7109.154997	8.660480	-0.046854	4.547633
224.527475	7117.173054	8.665485	-0.046881	4.550116
224.442606	7125.232880	8.670490	-0.046871	4.552610
225.107141	7133.255181	8.675495	-0.047001	4.555092
225.181489	7141.237330	8.680499	-0.047020	4.557560
225.258130	7149.222823	8.685504	-0.047040	4.560027
225.601462	7157.278316	8.690509	-0.047109	4.562515
225.486570	7165.263263	8.695514	-0.047093	4.564979
225.666032	7173.295926	8.700519	-0.047132	4.567457
225.806986	7181.297712	8.705523	-0.047164	4.569924
226.234134	7189.343461	8.710528	-0.047249	4.572404
226.287260	7197.363506	8.715533	-0.047265	4.574874
226.291244	7205.426618	8.720538	-0.047271	4.577355
226.443554	7213.402335	8.725543	-0.047305	4.579809
226.647288	7221.416798	8.730547	-0.047349	4.582273
226.667290	7229.394437	8.735552	-0.047358	4.584724
226.759510	7237.479918	8.740557	-0.047381	4.587208
226.933879	7245.433332	8.745562	-0.047419	4.589649
226.926565	7253.535932	8.750567	-0.047423	4.592135
227.146738	7261.509138	8.755571	-0.047469	4.594580
227.294161	7269.526531	8.760576	-0.047502	4.597037
227.527092	7277.507391	8.765581	-0.047551	4.599481
227.648407	7285.521275	8.770586	-0.047580	4.601934
227.935094	7293.517917	8.775591	-0.047638	4.604381
227.814215	7301.581492	8.780595	-0.047622	4.606847
228.085887	7309.496926	8.785600	-0.047678	4.609266
228.376761	7317.622113	8.790605	-0.047737	4.611748
228.529699	7325.643384	8.795610	-0.047772	4.614197
228.788581	7333.664905	8.800615	-0.047825	4.616645
228.819624	7341.646687	8.805619	-0.047837	4.619079
229.048129	7349.664562	8.810624	-0.047885	4.621523
229.056881	7357.623069	8.815629	-0.047892	4.623947
228.868743	7365.696351	8.820634	-0.047862	4.626406
229.125302	7373.723044	8.825639	-0.047916	4.628848
229.349766	7381.742750	8.830643	-0.047963	4.631287
229.443807	7389.764531	8.835648	-0.047986	4.633726
229.792212	7397.800262	8.840653	-0.048057	4.636167
229.763877	7405.718321	8.845658	-0.048057	4.638572
229.799755	7413.830960	8.850663	-0.048069	4.641034
229.957800	7421.770118	8.855667	-0.048104	4.643443
230.270234	7429.798303	8.860672	-0.048168	4.645877
230.321505	7437.786853	8.865677	-0.048183	4.648297
230.514428	7445.798559	8.870682	-0.048225	4.650724
230.877574	7453.919241	8.875687	-0.048298	4.653182
231.040273	7461.890961	8.880691	-0.048334	4.655594
231.122252	7469.863510	8.885696	-0.048354	4.658004
231.140469	7477.931954	8.890701	-0.048363	4.660443
231.188137	7485.916882	8.895706	-0.048378	4.662855
231.322657	7493.908390	8.900711	-0.048408	4.665268
231.452993	7501.949611	8.905715	-0.048438	4.667694
231.639140	7509.973578	8.910720	-0.048479	4.670114
231.935323	7518.041660	8.915725	-0.048539	4.672546
231.691222	7526.071051	8.920730	-0.048499	4.674965
232.061489	7534.073365	8.925735	-0.048574	4.677375
232.125264	7541.984986	8.930739	-0.048591	4.679756
232.289691	7550.039276	8.935744	-0.048628	4.682178
232.500737	7558.000439	8.940749	-0.048672	4.684572
232.672033	7566.068410	8.945754	-0.048710	4.686996
232.869200	7574.057612	8.950759	-0.048752	4.689395
232.720906	7582.094632	8.955763	-0.048730	4.691808
233.049672	7590.120038	8.960768	-0.048797	4.694216
233.260810	7598.189542	8.965773	-0.048842	4.696635
233.268966	7606.033761	8.970778	-0.048849	4.698986
233.307122	7614.161486	8.975783	-0.048862	4.701421
233.548733	7622.155147	8.980787	-0.048912	4.703814
233.669299	7630.158355	8.985792	-0.048940	4.706209
233.879926	7638.201867	8.990797	-0.048985	4.708615
234.096948	7646.199495	8.995802	-0.049031	4.711005
234.419371	7654.293032	9.000807	-0.049097	4.713423
234.208971	7662.267337	9.005811	-0.049063	4.715805
234.415964	7670.263714	9.010816	-0.049107	4.718191
234.604388	7678.280816	9.015821	-0.049148	4.720583
234.632820	7686.245172	9.020826	-0.049158	4.722958
234.942019	7694.314539	9.025831	-0.049222	4.725362
235.240590	7702.336681	9.030835	-0.049283	4.727751
235.219176	7710.335913	9.035840	-0.049284	4.730133
235.426126	7718.411646	9.040845	-0.049329	4.732535
235.521854	7726.370810	9.045850	-0.049352	4.734902
235.731504	7734.453823	9.050855	-0.049397	4.737305
235.688885	7742.426038	9.055859	-0.049394	4.739674
235.929851	7750.416708	9.060864	-0.049445	4.742046
236.245255	7758.464858	9.065869	-0.049509	4.744434
236.059993	7766.435030	9.070874	-0.049480	4.746799
236.080974	7774.439781	9.075879	-0.049489	4.749173
236.206925	7782.506607	9.080883	-0.049518	4.751564
236.530582	7790.547094	9.085888	-0.049584	4.753944
236.695121	7798.606802	9.090893	-0.049621	4.756330
236.733588	7806.488723	9.095898	-0.049633	4.758663
237.093832	7814.622209	9.100903	-0.049706	4.761067
236.989351	7822.536783	9.105907	-0.049692	4.763408
237.053933	7830.532312	9.110912	-0.049710	4.765770
237.543145	7838.600543	9.115917	-0.049806	4.768151
237.447134	7846.557736	9.120922	-0.049794	4.770500
237.653990	7854.645466	9.125927	-0.049838	4.772886
237.813883	7862.640360	9.130931	-0.049873	4.775243
238.188947	7870.679189	9.135936	-0.049949	4.777611
238.091537	7878.654364	9.140941	-0.049936	4.779961
238.244750	7886.701525	9.145946	-0.049970	4.782330
238.535971	7894.623074	9.150951	-0.050030	4.784660
238.772171	7902.695392	9.155955	-0.050080	4.787034
238.757447	7910.706665	9.160960	-0.050082	4.789389
238.987410	7918.779588	9.165965	-0.050131	4.791761
238.937105	7926.762166	9.170970	-0.050127	4.794106
239.277227	7934.821404	9.175975	-0.050196	4.796470
239.676629	7942.800507	9.180979	-0.050276	4.798810
239.814484	7950.796745	9.185984	-0.050307	4.801155
239.882403	7958.804404	9.190989	-0.050325	4.803502
239.869737	7966.789185	9.195994	-0.050328	4.805841
240.281269	7974.887955	9.200999	-0.050411	4.808211
240.258531	7982.883699	9.206003	-0.050412	4.810552
240.253919	7990.378779	9.211008	-0.050416	4.812745
240.530630	7994.930693	9.216013	-0.050471	4.814075

240.740453	7997.447505	9.221018	-0.050512	4.814810
240.685285	7998.840160	9.226023	-0.050503	4.815217
240.668922	7999.266013	9.231027	-0.050501	4.815342
240.829954	8000.273602	9.236032	-0.050532	4.815636
241.115627	8000.333832	9.241037	-0.050585	4.815652
241.129016	8000.282818	9.246042	-0.050588	4.815637
241.271127	8000.311868	9.251047	-0.050615	4.815645
241.059100	8000.329796	9.256051	-0.050576	4.815651
241.109151	8000.276176	9.261056	-0.050586	4.815635
241.475128	8000.341991	9.266061	-0.050654	4.815652
241.464929	8000.256415	9.271066	-0.050652	4.815627
241.356908	8000.274973	9.276071	-0.050633	4.815633
241.487196	8000.298491	9.281075	-0.050657	4.815640
241.751903	8000.270805	9.286080	-0.050707	4.815630
241.756098	8000.331779	9.291085	-0.050708	4.815648
241.781681	8000.292712	9.296090	-0.050713	4.815636
241.917006	8000.306700	9.301095	-0.050739	4.815640
241.754327	8000.320093	9.306099	-0.050709	4.815645
241.669625	8000.323012	9.311104	-0.050693	4.815646
241.861984	8000.269580	9.316109	-0.050730	4.815629
241.975188	8000.219128	9.321114	-0.050751	4.815614
241.812250	8000.231449	9.326119	-0.050721	4.815618
241.928325	8000.318815	9.331123	-0.050743	4.815643
241.982933	8000.235365	9.336128	-0.050753	4.815619
242.044941	8000.268448	9.341133	-0.050765	4.815628
241.951613	8000.265886	9.346138	-0.050748	4.815628
242.142385	8000.291461	9.351143	-0.050784	4.815634
242.313694	8000.324194	9.356147	-0.050816	4.815643
242.188824	8000.328592	9.361152	-0.050794	4.815645
242.200182	8000.311720	9.366157	-0.050796	4.815640
242.149580	8000.242571	9.371162	-0.050787	4.815620
242.118548	8000.285883	9.376167	-0.050781	4.815633
242.339892	8000.244672	9.381171	-0.050823	4.815620
242.423089	8000.264218	9.386176	-0.050839	4.815625
242.372836	8000.312556	9.391181	-0.050830	4.815639
242.189619	8000.273281	9.396186	-0.050796	4.815629
242.266806	8000.288456	9.401191	-0.050811	4.815633
242.413837	8000.296229	9.406195	-0.050839	4.815634
242.298499	8000.227090	9.411200	-0.050817	4.815615
242.466181	8000.277920	9.416205	-0.050849	4.815629
242.520678	8000.263889	9.421210	-0.050859	4.815624
242.395468	8000.305662	9.426215	-0.050836	4.815637
242.342004	8000.358219	9.431219	-0.050827	4.815653
242.539950	8000.317695	9.436224	-0.050864	4.815640
242.606168	8000.412794	9.441229	-0.050877	4.815667
242.699586	8000.349201	9.446234	-0.050895	4.815648
242.638764	8000.325809	9.451239	-0.050884	4.815642
242.883883	8000.295668	9.456243	-0.050929	4.815632
242.556913	8000.302104	9.461248	-0.050869	4.815635
242.589943	8000.373163	9.466253	-0.050875	4.815656
242.689057	8000.328888	9.471258	-0.050894	4.815642
242.887516	8000.306529	9.476263	-0.050932	4.815635
242.655191	8000.338007	9.481267	-0.050889	4.815645
242.770262	8000.270496	9.486272	-0.050910	4.815625
242.678536	8000.349130	9.491277	-0.050894	4.815648
242.553737	8000.318284	9.496282	-0.050871	4.815640
242.779860	8000.318805	9.501287	-0.050913	4.815639
242.914931	8000.315703	9.506291	-0.050939	4.815637
242.767139	8000.289821	9.511296	-0.050912	4.815631
242.884523	8000.324879	9.516301	-0.050934	4.815640
242.942403	8000.279930	9.521306	-0.050945	4.815627
242.970122	8000.296433	9.526311	-0.050950	4.815631
242.931759	8000.390892	9.531315	-0.050944	4.815659
242.960294	8000.324102	9.536320	-0.050949	4.815640
243.136105	8000.380408	9.541325	-0.050982	4.815655
242.885049	8000.299436	9.546330	-0.050936	4.815633
243.061477	8000.291670	9.551335	-0.050969	4.815630
243.026395	8000.316759	9.556339	-0.050963	4.815637
242.981572	8000.265859	9.561344	-0.050955	4.815622
243.169904	8000.329846	9.566349	-0.050990	4.815640
242.960823	8000.269853	9.571354	-0.050952	4.815624
243.092817	8000.269904	9.576359	-0.050977	4.815623
243.001360	8000.331454	9.581363	-0.050960	4.815641
243.143519	8000.301767	9.586368	-0.050987	4.815632
243.208195	8000.350916	9.591373	-0.050999	4.815646
243.055946	8000.288648	9.596378	-0.050971	4.815629
243.036871	8000.299046	9.601383	-0.050968	4.815632
243.349096	8000.333017	9.606387	-0.051026	4.815640
243.387507	8000.303770	9.611392	-0.051034	4.815631
243.330031	8000.327426	9.616397	-0.051024	4.815639
243.309821	8000.272656	9.621402	-0.051020	4.815623
243.472242	8000.299906	9.626407	-0.051051	4.815630
243.519223	8000.307112	9.631411	-0.051060	4.815632
243.306860	8000.309012	9.636416	-0.051021	4.815633
243.409477	8000.326740	9.641421	-0.051040	4.815638
243.194498	8000.312576	9.646426	-0.051000	4.815635
243.286643	8000.268186	9.651431	-0.051018	4.815621
243.459351	8000.297741	9.656435	-0.051050	4.815629
243.462913	8000.285013	9.661440	-0.051051	4.815626
243.556245	8000.313270	9.666445	-0.051069	4.815633
243.379360	8000.313613	9.671450	-0.051037	4.815634
243.528587	8000.255204	9.676455	-0.051065	4.815616
243.406181	8000.274594	9.681459	-0.051042	4.815623
243.495710	8000.273952	9.686464	-0.051059	4.815622
243.805963	8000.324980	9.691469	-0.051117	4.815636
243.591769	8000.258494	9.696474	-0.051078	4.815617
243.545090	8000.296211	9.701479	-0.051070	4.815628
243.669083	8000.336718	9.706483	-0.051093	4.815640
243.776385	8000.235969	9.711488	-0.051113	4.815610
243.698681	8000.282792	9.716493	-0.051099	4.815624
243.551125	8000.234484	9.721498	-0.051072	4.815610
243.803041	8000.276014	9.726503	-0.051119	4.815621
243.659572	8000.272631	9.731507	-0.051093	4.815621
243.557396	8000.260310	9.736512	-0.051074	4.815618
243.994255	8000.314477	9.741517	-0.051156	4.815631
243.762985	8000.298977	9.746522	-0.051113	4.815628
243.616544	8000.343608	9.751527	-0.051086	4.815642
243.719876	8000.366689	9.756531	-0.051106	4.815648
243.774237	8000.278959	9.761536	-0.051116	4.815622
243.776883	8000.311074	9.766541	-0.051117	4.815631
243.678667	8000.372514	9.771546	-0.051099	4.815650
243.803981	8000.275264	9.776551	-0.051123	4.815621
243.766661	8000.355857	9.781555	-0.051116	4.815645
243.714690	8000.318723	9.786560	-0.051107	4.815634
243.862811	8000.404484	9.791565	-0.051135	4.815658
243.802524	8000.288178	9.796570	-0.051124	4.815625
243.853001	8000.269809	9.801575	-0.051134	4.815619
243.773609	8000.297379	9.806579	-0.051119	4.815627
243.721578	8000.269857	9.811584	-0.051110	4.815620
243.630274	8000.272667	9.816589	-0.051093	4.815621
243.615005	8000.280992	9.821594	-0.051091	4.815623
243.916871	8000.370334	9.826599	-0.051147	4.815648
243.860409	8000.328855	9.831603	-0.051137	4.815636
243.693332	8000.273819	9.836608	-0.051106	4.815621
243.946985	8000.335671	9.841613	-0.051154	4.815638
243.891956	8000.281399	9.846618	-0.051144	4.815622
243.751683	8000.307973	9.851623	-0.051118	4.815631
243.852170	8000.282945	9.856627	-0.051137	4.815623
243.915674	8000.202841	9.861632	-0.051149	4.815599
244.114070	8000.258450	9.866637	-0.051187	4.815614
243.887179	8000.212049	9.871642	-0.051145	4.815602
244.092944	8000.265642	9.876647	-0.051184	4.815616
244.141396	8000.286758	9.881651	-0.051193	4.815622
243.844676	8000.280868	9.886656	-0.051138	4.815622
243.850895	8000.324791	9.891661	-0.051140	4.815635
243.994042	8000.327161	9.896666	-0.051167	4.815635
244.030339	8000.273314	9.901671	-0.051174	4.815619
243.975902	8000.349355	9.906675	-0.051164	4.815641
244.075367	8000.271975	9.911680	-0.051183	4.815618
244.017775	8000.321262	9.916685	-0.051172	4.815633
244.106507	8000.249047	9.921690	-0.051189	4.815611
244.050737	8000.279139	9.926695	-0.051179	4.815621
244.055314	8000.328375	9.931699	-0.051180	4.815635
243.924625	8000.281410	9.936704	-0.051156	4.815622
244.061081	8000.346687	9.941709	-0.051182	4.815640
244.104234	8000.317518	9.946714	-0.051191	4.815631
244.078890	8000.292568	9.951719	-0.051186	4.815624
244.145127	8000.344949	9.956723	-0.051199	4.815639
243.974177	8000.333639	9.961728	-0.051167	4.815637
244.154366	8000.441287	9.966733	-0.051201	4.815667
243.939488	8000.398284	9.971738	-0.051162	4.815656
243.980332	8000.355192	9.976743	-0.051170	4.815643
244.158878	8000.341053	9.981747	-0.051203	4.815638
244.073424	8000.296963	9.986752	-0.051188	4.815626
244.106117	8000.351999	9.991757	-0.051194	4.815641
244.125659	8000.294673	9.996762	-0.051198	4.815625
244.300602	8000.329607	10.001767	-0.051231	4.815634
244.221128	8000.343290	10.006771	-0.051216	4.815638
244.128604	8000.312970	10.011776	-0.051200	4.815630
244.439290	8000.329830	10.016781	-0.051258	4.815633
244.089708	8000.314530	10.021786	-0.051193	4.815631
244.182725	8000.327830	10.026791	-0.051211	4.815634
244.361672	8000.401280	10.031795	-0.051244	4.815655
244.157115	8000.291158	10.036800	-0.051207	4.815623
244.197245	8000.347384	10.041805	-0.051214	4.815640
244.098075	8000.359677	10.046810	-0.051196	4.815644
244.109930	8000.320383	10.051815	-0.051199	4.815632
244.241749	8000.325773	10.056819	-0.051224	4.815633
244.107306	8000.265929	10.061824	-0.051199	4.815616
244.282215	8000.310475	10.066829	-0.051232	4.815628
244.121729	8000.303608	10.071834	-0.051202	4.815627
244.139767	8000.279368	10.076839	-0.051206	4.815620
244.276791	8000.316885	10.081843	-0.051232	4.815630
244.251540	8000.295141	10.086848	-0.051228	4.815624
244.179027	8000.318551	10.091853	-0.051214	4.815631
244.277520	8000.302035	10.096858	-0.051233	4.815626
244.432900	8000.312083	10.101863	-0.051262	4.815628
244.376899	8000.318674	10.106867	-0.051252	4.815630
244.382953	8000.237630	10.111872	-0.051254	4.815606
244.555691	8000.370790	10.116877	-0.051286	4.815645
244.417701	8000.321568	10.121882	-0.051261	4.815631
244.360056	8000.318520	10.126887	-0.051251	4.815630
244.469189	8000.383351	10.131891	-0.051271	4.815649
244.371485	8000.268568	10.136896	-0.051253	4.815616
244.316030	8000.358477	10.141901	-0.051243	4.815642
244.304488	8000.312392	10.146906	-0.051242	4.815629
244.321680	8000.335133	10.151911	-0.051245	4.815635
244.395154	8000.340637	10.156915	-0.051259	4.815636
244.394417	8000.269094	10.161920	-0.051259	4.815616
244.677436	8000.361336	10.166925	-0.051312	4.815641
244.573786	8000.321220	10.171930	-0.051293	4.815630
244.404337	8000.270415	10.176935	-0.051262	4.815616
244.397728	8000.386758	10.181939	-0.051261	4.815650
244.394168	8000.350415	10.186944	-0.051261	4.815639
244.497282	8000.368153	10.191949	-0.051281	4.815644
244.385122	8000.341783	10.196954	-0.051260	4.815637
244.575906	8000.311824	10.201959	-0.051296	4.815627
244.537793	8000.364635	10.206963	-0.051289	4.815643
244.349463	8000.274002	10.211968	-0.051254	4.815617
244.479717	8000.314614	10.216973	-0.051279	4.815628
244.505495	8000.279819	10.221978	-0.051284	4.815618
244.545961	8000.344596	10.226983	-0.051292	4.815637
244.533566	8000.385011	10.231987	-0.051290	4.815649
244.665066	8000.369035	10.236992	-0.051315	4.815643
244.614229	8000.374642	10.241997	-0.051306	4.815645
244.459484	8000.381754	10.247002	-0.051277	4.815648
244.505283	8000.322721	10.252007	-0.051286	4.815631
244.621990	8000.364179	10.257011	-0.051308	4.815642
244.558432	8000.299085	10.262016	-0.051297	4.815623
244.686052	8000.381309	10.267021	-0.051321	4.815647
244.628074	8000.368642	10.272026	-0.051311	4.815643
244.755222	8000.338709	10.277031	-0.051335	4.815634
244.765229	8000.333563	10.282035	-0.051337	4.815632
244.869425	8000.379089	10.287040	-0.051357	4.815645
244.633260	8000.414775	10.292045	-0.051313	4.815657
244.796110	8000.379019	10.297050	-0.051344	4.815646
244.796001	8000.322438	10.302055	-0.051344	4.815629
244.871328	8000.360016	10.307059	-0.051358	4.815640
244.795933	8000.278706	10.312064	-0.051344	4.815616
244.871054	8000.367549	10.317069	-0.051359	4.815642
244.616563	8000.369824	10.322074	-0.051312	4.815644
244.569187	8000.351990	10.327079	-0.051303	4.815639
244.869859	8000.393254	10.332083	-0.051360	4.815649
244.717128	8000.341654	10.337088	-0.051332	4.815635
244.789580	8000.377048	10.342093	-0.051345	4.815645
244.893645	8000.370236	10.347098	-0.051365	4.815642
244.965757	8000.256093	10.352103	-0.051379	4.815609
244.967478	8000.357620	10.357107	-0.051380	4.815638
245.011567	8000.308171	10.362112	-0.051388	4.815624
245.062153	8000.341072	10.367117	-0.051398	4.815633
244.961830	8000.293533	10.372122	-0.051380	4.815620
245.085190	8000.305194	10.377127	-0.051403	4.815622
245.085250	8000.342609	10.382131	-0.051403	4.815633
244.959407	8000.288244	10.387136	-0.051380	4.815618
245.129548	8000.355143	10.392141	-0.051412	4.815637
244.956858	8000.324578	10.397146	-0.051380	4.815629
244.976086	8000.267246	10.402151	-0.051384	4.815612
244.945915	8000.334072	10.407155	-0.051379	4.815631
244.945091	8000.302046	10.412160	-0.051379	4.815622
244.824683	8000.356715	10.417165	-0.051357	4.815639
245.019617	8000.353526	10.422170	-0.051394	4.815637
244.964139	8000.262929	10.427175	-0.051384	4.815611
245.129938	8000.290238	10.432179	-0.051415	4.815618
244.998946	8000.284921	10.437184	-0.051391	4.815617
244.940853	8000.305363	10.442189	-0.051380	4.815623
244.800598	8000.281737	10.447194	-0.051355	4.815617
244.987007	8000.289089	10.452199	-0.051390	4.815618
244.972299	8000.286743	10.457203	-0.051387	4.815617
244.719106	8000.292244	10.462208	-0.051341	4.815620
244.930238	8000.332043	10.467213	-0.051380	4.815631
244.918407	8000.270999	10.472218	-0.051378	4.815613
244.833956	8000.247218	10.477223	-0.051363	4.815606
245.021170	8000.361392	10.482227	-0.051398	4.815639
244.915263	8000.337260	10.487232	-0.051379	4.815632
245.189372	8000.422951	10.492237	-0.051430	4.815656
245.124665	8000.379198	10.497242	-0.051419	4.815644
244.992950	8000.310851	10.502247	-0.051394	4.815624
245.202222	8000.335667	10.507251	-0.051434	4.815631
245.127388	8000.318452	10.512256	-0.051420	4.815626
245.209021	8000.358269	10.517261	-0.051436	4.815637
245.168068	8000.346949	10.522266	-0.051428	4.815634
245.049856	8000.335432	10.527271	-0.051407	4.815631
245.026252	8000.359642	10.532275	-0.051403	4.815638
244.950861	8000.307171	10.537280	-0.051389	4.815623
245.179178	8000.377158	10.542285	-0.051432	4.815643
244.951774	8000.357447	10.547290	-0.051390	4.815638
245.115511	8000.337726	10.552295	-0.051421	4.815631
245.066627	8000.346569	10.557299	-0.051412	4.815634
244.887111	8000.260352	10.562304	-0.051379	4.815610
245.111891	8000.360188	10.567309	-0.051421	4.815638
245.197296	8000.310346	10.572314	-0.051437	4.815623
245.088777	8000.313942	10.577319	-0.051417	4.815625
245.058999	8000.313485	10.582323	-0.051412	4.815625
245.419309	8000.291640	10.587328	-0.051480	4.815616
245.180046	8000.299505	10.592333	-0.051435	4.815620
245.122252	8000.286840	10.597338	-0.051425	4.815616
245.254983	8000.278361	10.602343	-0.051450	4.815613
245.373699	8000.292083	10.607347	-0.051472	4.815617
245.265263	8000.309565	10.612352	-0.051453	4.815622
245.233557	8000.305872	10.617357	-0.051447	4.815621
245.154914	8000.374042	10.622362	-0.051433	4.815642
245.265023	8000.369466	10.627367	-0.051454	4.815640
245.272294	8000.374955	10.632371	-0.051455	4.815641
245.168513	8000.342313	10.637376	-0.051436	4.815632
245.232871	8000.385052	10.642381	-0.051449	4.815645
244.963795	8000.399905	10.647386	-0.051399	4.815650
245.116455	8000.334075	10.652391	-0.051428	4.815630
245.211160	8000.374107	10.657395	-0.051446	4.815641
245.114732	8000.268954	10.662400	-0.051428	4.815611
245.293911	8000.365908	10.667405	-0.051462	4.815639
245.295007	8000.346731	10.672410	-0.051462	4.815633
245.257220	8000.291670	10.677415	-0.051456	4.815617
245.270011	8000.366676	10.682419	-0.051458	4.815639
245.214425	8000.284622	10.687424	-0.051448	4.815615
245.349510	8000.344540	10.692429	-0.051474	4.815632
245.306749	8000.325712	10.697434	-0.051466	4.815627
245.375766	8000.309782	10.702439	-0.051479	4.815622
245.373012	8000.350356	10.707443	-0.051479	4.815634
245.482563	8000.310522	10.712448	-0.051500	4.815621
245.411262	8000.316863	10.717453	-0.051487	4.815624
245.476125	8000.327567	10.722458	-0.051499	4.815626
245.507827	8000.314231	10.727463	-0.051506	4.815622
245.280741	8000.353270	10.732467	-0.051464	4.815635
245.155408	8000.348045	10.737472	-0.051441	4.815634
245.414760	8000.360864	10.742477	-0.051489	4.815636
245.276972	8000.366116	10.747482	-0.051464	4.815639
245.186281	8000.298440	10.752487	-0.051448	4.815619
245.399209	8000.363905	10.757491	-0.051488	4.815637
245.434481	8000.303630	10.762496	-0.051494	4.815620
245.388322	8000.372332	10.767501	-0.051486	4.815640
245.463510	8000.352231	10.772506	-0.051501	4.815634
245.615447	8000.328045	10.777511	-0.051529	4.815626
245.654615	8000.397075	10.782515	-0.051537	4.815646
245.446855	8000.311461	10.787520	-0.051498	4.815622
245.539446	8000.379229	10.792525	-0.051516	4.815641
245.568820	8000.372264	10.797530	-0.051522	4.815639
245.539946	8000.330165	10.802535	-0.051517	4.815627
245.557712	8000.383892	10.807539	-0.051521	4.815642
245.416211	8000.297226	10.812544	-0.051494	4.815618
245.340797	8000.333406	10.817549	-0.051481	4.815629
245.460453	8000.333258	10.822554	-0.051503	4.815628
245.521225	8000.277673	10.827559	-0.051515	4.815611
245.443570	8000.392856	10.832563	-0.051501	4.815646
245.286284	8000.377496	10.837568	-0.051472	4.815642
245.543630	8000.327264	10.842573	-0.051520	4.815626
245.457835	8000.335503	10.847578	-0.051505	4.815629
245.487819	8000.341364	10.852583	-0.051511	4.815630
245.542686	8000.393562	10.857587	-0.051521	4.815645
245.436188	8000.366215	10.862592	-0.051502	4.815638
245.422255	8000.411946	10.867597	-0.051499	4.815651
245.456685	8000.375156	10.872602	-0.051506	4.815640
245.434301	8000.342776	10.877607	-0.051502	4.815631
245.358251	8000.351175	10.882611	-0.051489	4.815634
245.321051	8000.330303	10.887616	-0.051482	4.815628
245.609205	8000.325436	10.892621	-0.051536	4.815625
245.385233	8000.358116	10.897626	-0.051495	4.815636
245.314741	8000.343108	10.902631	-0.051482	4.815631
245.446301	8000.295090	10.907635	-0.051507	4.815617
245.535901	8000.311540	10.912640	-0.051524	4.815621
245.494862	8000.347214	10.917645	-0.051516	4.815632
245.632492	8000.323862	10.922650	-0.051542	4.815624
245.622009	8000.311972	10.927655	-0.051541	4.815621
245.649759	8000.327410	10.932659	-0.051546	4.815625
245.645032	8000.317750	10.937664	-0.051546	4.815622
245.815386	8000.383587	10.942669	-0.051578	4.815641
245.789784	8000.372517	10.947674	-0.051573	4.815638
245.668761	8000.310752	10.952679	-0.051551	4.815620
245.490424	8000.351657	10.957683	-0.051518	4.815633
245.484649	8000.327026	10.962688	-0.051518	4.815626
245.766325	8000.361573	10.967693	-0.051570	4.815635
245.605839	8000.317321	10.972698	-0.051541	4.815622
245.524460	8000.306406	10.977703	-0.051526	4.815620
245.659908	8000.344969	10.982707	-0.051552	4.815630
245.495646	8000.309200	10.987712	-0.051521	4.815621
245.761379	8000.340282	10.992717	-0.051571	4.815628
245.637214	8000.330803	10.997722	-0.051548	4.815626
245.778275	8000.292554	11.002727	-0.051575	4.815614
245.841777	8000.370528	11.007731	-0.051587	4.815637
245.876947	8000.256845	11.012736	-0.051594	4.815603
245.852703	8000.299203	11.017741	-0.051590	4.815616
245.755816	8000.347850	11.022746	-0.051572	4.815631
245.721561	8000.301390	11.027751	-0.051566	4.815617
245.818201	8000.290185	11.032755	-0.051585	4.815613
245.485086	8000.263402	11.037760	-0.051523	4.815607
245.528479	8000.315411	11.042765	-0.051531	4.815622
245.678511	8000.333919	11.047770	-0.051560	4.815627
245.430483	8000.293574	11.052775	-0.051514	4.815616
245.726253	8000.373213	11.057779	-0.051569	4.815638
245.721806	8000.298402	11.062784	-0.051569	4.815616
245.842323	8000.396536	11.067789	-0.051591	4.815644
245.703659	8000.322732	11.072794	-0.051566	4.815623
245.701952	8000.333416	11.077799	-0.051566	4.815626
245.911448	8000.361442	11.082803	-0.051605	4.815634
245.633472	8000.306721	11.087808	-0.051554	4.815619
245.575203	8000.295117	11.092813	-0.051543	4.815616
245.684967	8000.261696	11.097818	-0.051564	4.815606
245.771401	8000.254596	11.102823	-0.051581	4.815603
245.814199	8000.341844	11.107827	-0.051589	4.815628
245.706706	8000.277096	11.112832	-0.051569	4.815610
245.732543	8000.307456	11.117837	-0.051574	4.815619
245.527291	8000.321217	11.122842	-0.051537	4.815624
245.681810	8000.292801	11.127847	-0.051566	4.815615
245.711267	8000.396921	11.132851	-0.051572	4.815645
245.713388	8000.376692	11.137856	-0.051572	4.815639
245.666110	8000.383425	11.142861	-0.051564	4.815641
245.795556	8000.333236	11.147866	-0.051588	4.815626
245.783172	8000.310633	11.152871	-0.051586	4.815619
245.827227	8000.330611	11.157875	-0.051595	4.815625
245.727589	8000.304444	11.162880	-0.051577	4.815618
245.893239	8000.426815	11.167885	-0.051608	4.815653
245.724943	8000.420886	11.172890	-0.051577	4.815652
245.773848	8000.305292	11.177895	-0.051586	4.815618
245.901052	8000.266816	11.182899	-0.051610	4.815606
245.727505	8000.278959	11.187904	-0.051578	4.815610
245.743676	8000.309161	11.192909	-0.051582	4.815619
245.944163	8000.291111	11.197914	-0.051619	4.815613
245.774306	8000.289429	11.202919	-0.051588	4.815613
245.852197	8000.358026	11.207923	-0.051603	4.815633
245.659855	8000.275868	11.212928	-0.051567	4.815610
246.084809	8000.362962	11.217933	-0.051647	4.815633
245.776996	8000.382521	11.222938	-0.051590	4.815640
245.757494	8000.312804	11.227943	-0.051587	4.815620
245.918249	8000.366736	11.232947	-0.051617	4.815635
245.843067	8000.321742	11.237952	-0.051603	4.815622
245.849785	8000.358199	11.242957	-0.051605	4.815633
245.832060	8000.416686	11.247962	-0.051602	4.815650
245.867976	8000.374579	11.252967	-0.051609	4.815637
245.923004	8000.403281	11.257971	-0.051620	4.815646
245.843746	8000.302679	11.262976	-0.051605	4.815616
245.861208	8000.345720	11.267981	-0.051609	4.815629
245.856713	8000.374516	11.272986	-0.051608	4.815637
245.992895	8000.345800	11.277991	-0.051634	4.815628
246.023336	8000.400803	11.282995	-0.051640	4.815644
245.876416	8000.320455	11.288000	-0.051613	4.815621
245.872763	8000.348197	11.293005	-0.051613	4.815630
245.841982	8000.349860	11.298010	-0.051607	4.815630
245.862456	8000.280797	11.303015	-0.051611	4.815610
245.781661	8000.342524	11.308019	-0.051597	4.815628
245.826296	8000.316582	11.313024	-0.051605	4.815621
245.982538	8000.365099	11.318029	-0.051635	4.815634
245.983626	8000.363011	11.323034	-0.051635	4.815633
245.869752	8000.324861	11.328039	-0.051614	4.815623
246.121058	8000.420865	11.333043	-0.051662	4.815650
246.133295	8000.302533	11.338048	-0.051664	4.815615
246.127962	8000.308884	11.343053	-0.051664	4.815617
246.085223	8000.380848	11.348058	-0.051656	4.815638
246.131640	8000.354935	11.353063	-0.051665	4.815630
246.171871	8000.389804	11.358067	-0.051673	4.815640
246.061720	8000.365600	11.363072	-0.051653	4.815634
246.199744	8000.424501	11.368077	-0.051679	4.815650
246.018674	8000.407682	11.373082	-0.051645	4.815646
245.881324	8000.377692	11.378087	-0.051620	4.815638
246.018416	8000.418419	11.383091	-0.051646	4.815649
245.901607	8000.402652	11.388096	-0.051625	4.815645
246.041644	8000.425269	11.393101	-0.051651	4.815651
245.949831	8000.401366	11.398106	-0.051634	4.815645
246.072574	8000.312614	11.403111	-0.051657	4.815618
246.083045	8000.384381	11.408115	-0.051660	4.815639
246.140824	8000.323405	11.413120	-0.051671	4.815621
246.281167	8000.370595	11.418125	-0.051697	4.815634
246.243661	8000.377488	11.423130	-0.051691	4.815636
246.003406	8000.406697	11.428135	-0.051646	4.815646
245.964660	8000.430660	11.433139	-0.051639	4.815653
245.965940	8000.411485	11.438144	-0.051640	4.815647
246.034515	8000.401957	11.443149	-0.051653	4.815644
245.978281	8000.392521	11.448154	-0.051643	4.815642
246.048686	8000.279415	11.453159	-0.051656	4.815608
246.113404	8000.339251	11.458163	-0.051669	4.815626
245.973321	8000.288923	11.463168	-0.051643	4.815611
246.069916	8000.312965	11.468173	-0.051661	4.815618
246.225978	8000.360412	11.473178	-0.051691	4.815631
246.040051	8000.309332	11.478183	-0.051657	4.815617
246.217808	8000.393451	11.483187	-0.051690	4.815641
246.231890	8000.354191	11.488192	-0.051693	4.815629
246.170960	8000.391676	11.493197	-0.051682	4.815641
246.193122	8000.379252	11.498202	-0.051686	4.815637
246.169394	8000.296647	11.503207	-0.051682	4.815613
246.462133	8000.396535	11.508211	-0.051737	4.815641
246.125125	8000.373957	11.513216	-0.051675	4.815636
246.201257	8000.406210	11.518221	-0.051689	4.815645
246.249440	8000.384598	11.523226	-0.051699	4.815638
246.103324	8000.321353	11.528231	-0.051672	4.815620
246.190421	8000.424282	11.533235	-0.051688	4.815650
246.178808	8000.376056	11.538240	-0.051687	4.815636
246.134498	8000.335840	11.543245	-0.051679	4.815624
246.124704	8000.336778	11.548250	-0.051677	4.815625
246.234558	8000.292677	11.553255	-0.051698	4.815611
246.314072	8000.331394	11.558259	-0.051713	4.815622
246.130346	8000.302781	11.563264	-0.051679	4.815615
246.377064	8000.332486	11.568269	-0.051726	4.815622
246.272774	8000.325468	11.573274	-0.051706	4.815621
246.231514	8000.371821	11.578279	-0.051699	4.815634
246.305946	8000.373070	11.583283	-0.051713	4.815634
246.270849	8000.365048	11.588288	-0.051707	4.815632
246.391478	8000.356372	11.593293	-0.051730	4.815629
246.203620	8000.400325	11.598298	-0.051695	4.815643
246.379240	8000.354096	11.603303	-0.051728	4.815628
246.419100	8000.419936	11.608307	-0.051736	4.815647
246.267292	8000.366210	11.613312	-0.051708	4.815632
246.286498	8000.375100	11.618317	-0.051712	4.815635
246.337005	8000.378093	11.623322	-0.051722	4.815636
246.077338	8000.332215	11.628327	-0.051674	4.815623
246.222884	8000.345310	11.633331	-0.051701	4.815626
246.046152	8000.361673	11.638336	-0.051669	4.815632
246.354713	8000.394527	11.643341	-0.051727	4.815640
246.263316	8000.364221	11.648346	-0.051710	4.815632
246.335248	8000.376110	11.653351	-0.051724	4.815635
246.296634	8000.392599	11.658355	-0.051717	4.815640
246.269643	8000.336644	11.663360	-0.051712	4.815624
246.229389	8000.334947	11.668365	-0.051705	4.815623
246.250062	8000.343861	11.673370	-0.051709	4.815626
246.073244	8000.384790	11.678375	-0.051677	4.815639
246.270195	8000.336774	11.683379	-0.051714	4.815624
246.515925	8000.326942	11.688384	-0.051760	4.815620
246.286444	8000.391576	11.693389	-0.051717	4.815640
246.228291	8000.339384	11.698394	-0.051707	4.815625
246.233739	8000.304255	11.703399	-0.051708	4.815614
246.220768	8000.382047	11.708403	-0.051706	4.815637
246.196064	8000.421194	11.713408	-0.051702	4.815649
246.421457	8000.360826	11.718413	-0.051744	4.815630
246.345827	8000.406616	11.723418	-0.051730	4.815644
246.321534	8000.343229	11.728423	-0.051726	4.815625
246.499576	8000.435898	11.733427	-0.051760	4.815651
246.339411	8000.344650	11.738432	-0.051730	4.815626
246.426115	8000.387758	11.743437	-0.051747	4.815638
246.466117	8000.375625	11.748442	-0.051755	4.815634
246.439826	8000.351726	11.753447	-0.051750	4.815627
246.604780	8000.366207	11.758451	-0.051781	4.815631
246.458792	8000.386278	11.763456	-0.051754	4.815637
246.401964	8000.359742	11.768461	-0.051744	4.815630
246.518210	8000.397993	11.773466	-0.051766	4.815640
246.403179	8000.360891	11.778471	-0.051745	4.815630
246.405933	8000.339603	11.783475	-0.051746	4.815624
246.356107	8000.370862	11.788480	-0.051737	4.815633
246.521199	8000.428071	11.793485	-0.051768	4.815649
246.211496	8000.403804	11.798490	-0.051711	4.815643
246.555845	8000.398791	11.803495	-0.051775	4.815640
246.558046	8000.438379	11.808499	-0.051776	4.815652
246.323153	8000.387565	11.813504	-0.051732	4.815638
246.227613	8000.380690	11.818509	-0.051715	4.815636
246.405789	8000.434909	11.823514	-0.051749	4.815651
246.367062	8000.431100	11.828519	-0.051742	4.815651
246.500381	8000.449336	11.833523	-0.051767	4.815655
246.446748	8000.407898	11.838528	-0.051757	4.815643
246.592657	8000.437022	11.843533	-0.051785	4.815651
246.458480	8000.473308	11.848538	-0.051760	4.815662
246.408234	8000.422313	11.853543	-0.051751	4.815648
246.521139	8000.457305	11.858547	-0.051772	4.815657
246.198513	8000.427485	11.863552	-0.051713	4.815650
246.250158	8000.457200	11.868557	-0.051723	4.815659
246.271650	8000.456515	11.873562	-0.051727	4.815658
246.304437	8000.402606	11.878567	-0.051733	4.815642
246.376818	8000.428389	11.883571	-0.051747	4.815650
246.273206	8000.362635	11.888576	-0.051728	4.815631
246.397786	8000.422385	11.893581	-0.051752	4.815648
246.311071	8000.446630	11.898586	-0.051736	4.815655
246.253138	8000.421145	11.903591	-0.051726	4.815648
246.433357	8000.438012	11.908595	-0.051760	4.815652
246.369272	8000.426312	11.913600	-0.051748	4.815649
246.465477	8000.419372	11.918605	-0.051766	4.815646
246.411893	8000.446297	11.923610	-0.051757	4.815655
246.425796	8000.368580	11.928615	-0.051759	4.815632
246.494544	8000.466938	11.933619	-0.051773	4.815660
246.348881	8000.386608	11.938624	-0.051746	4.815637
246.284115	8000.352465	11.943629	-0.051734	4.815628
246.338263	8000.370473	11.948634	-0.051745	4.815633
246.349427	8000.334369	11.953639	-0.051747	4.815622
246.692904	8000.428680	11.958643	-0.051811	4.815648
246.408810	8000.363174	11.963648	-0.051759	4.815630
246.159925	8000.350584	11.968653	-0.051713	4.815628
246.334576	8000.386586	11.973658	-0.051746	4.815637
246.568337	8000.330628	11.978663	-0.051789	4.815620
246.495641	8000.421329	11.983667	-0.051776	4.815647
246.395583	8000.357768	11.988672	-0.051758	4.815629
246.453998	8000.414298	11.993677	-0.051769	4.815645
246.468133	8000.449809	11.998682	-0.051772	4.815655
246.367963	8000.313613	12.003687	-0.051754	4.815616
246.724008	8000.432697	12.008691	-0.051821	4.815649
246.724273	8000.433800	12.013696	-0.051821	4.815649
246.559772	8000.376661	12.018701	-0.051791	4.815633
246.606567	8000.437274	12.023706	-0.051800	4.815651
246.548338	8000.428874	12.028711	-0.051789	4.815649
246.684995	8000.436483	12.033715	-0.051815	4.815650
246.499308	8000.324521	12.038720	-0.051781	4.815618
246.664228	8000.378523	12.043725	-0.051812	4.815633
246.648502	8000.449862	12.048730	-0.051809	4.815654
246.362084	8000.367227	12.053735	-0.051756	4.815631
246.573133	8000.438007	12.058739	-0.051796	4.815651
246.688065	8000.305332	12.063744	-0.051818	4.815612
246.537127	8000.340276	12.068749	-0.051790	4.815623
246.526584	8000.405291	12.073754	-0.051788	4.815642
246.554442	8000.322462	12.078759	-0.051794	4.815617
246.475365	8000.454716	12.083763	-0.051779	4.815656
246.471424	8000.347867	12.088768	-0.051779	4.815625
246.636561	8000.339920	12.093773	-0.051810	4.815622
246.727931	8000.396991	12.098778	-0.051827	4.815638
246.566712	8000.352723	12.103783	-0.051798	4.815626
246.535504	8000.423808	12.108787	-0.051792	4.815647
246.420739	8000.363211	12.113792	-0.051771	4.815630
246.782468	8000.430050	12.118797	-0.051839	4.815648
246.647345	8000.482343	12.123802	-0.051814	4.815664
246.538294	8000.435725	12.128807	-0.051794	4.815651
246.536894	8000.448550	12.133811	-0.051794	4.815654
246.460620	8000.378970	12.138816	-0.051780	4.815634
246.572315	8000.362671	12.143821	-0.051802	4.815629
246.696915	8000.387173	12.148826	-0.051825	4.815636
246.531953	8000.349253	12.153831	-0.051795	4.815625
246.531256	8000.378112	12.158835	-0.051795	4.815634
246.564818	8000.357328	12.163840	-0.051802	4.815627
246.713937	8000.367278	12.168845	-0.051830	4.815630
246.340700	8000.396445	12.173850	-0.051761	4.815640
246.495526	8000.325309	12.178855	-0.051790	4.815618
246.489010	8000.370094	12.183859	-0.051789	4.815631
246.259073	8000.393063	12.188864	-0.051746	4.815639
246.323337	8000.402691	12.193869	-0.051759	4.815642
246.509911	8000.385482	12.198874	-0.051794	4.815636
246.573688	8000.369466	12.203879	-0.051806	4.815631
246.453864	8000.414533	12.208883	-0.051784	4.815645
246.511037	8000.451817	12.213888	-0.051795	4.815655
246.582235	8000.418832	12.218893	-0.051809	4.815645
246.746025	8000.481362	12.223898	-0.051840	4.815663
246.643243	8000.372893	12.228903	-0.051821	4.815631
246.921319	8000.418068	12.233907	-0.051873	4.815643
246.657759	8000.383873	12.238912	-0.051824	4.815635
246.812137	8000.321274	12.243917	-0.051853	4.815616
246.955673	8000.451835	12.248922	-0.051880	4.815653
246.482726	8000.443051	12.253927	-0.051793	4.815653
246.529210	8000.472682	12.258931	-0.051802	4.815661
246.627485	8000.413437	12.263936	-0.051820	4.815643
246.594739	8000.430022	12.268941	-0.051814	4.815648
246.591416	8000.438543	12.273946	-0.051814	4.815651
246.499820	8000.375120	12.278951	-0.051797	4.815633
246.638389	8000.360330	12.283955	-0.051824	4.815628
246.593787	8000.380993	12.288960	-0.051816	4.815634
246.565853	8000.347453	12.293965	-0.051811	4.815624
246.663032	8000.436663	12.298970	-0.051829	4.815650
246.820875	8000.371985	12.303975	-0.051859	4.815630
246.694722	8000.458606	12.308979	-0.051836	4.815656
246.655562	8000.459063	12.313984	-0.051829	4.815656
246.693325	8000.330465	12.318989	-0.051836	4.815619
246.849507	8000.358689	12.323994	-0.051866	4.815626
246.775601	8000.308374	12.328999	-0.051852	4.815612
246.883820	8000.372130	12.334003	-0.051873	4.815630
246.647004	8000.324487	12.339008	-0.051829	4.815617
246.693661	8000.364803	12.344013	-0.051838	4.815629
246.627835	8000.401141	12.349018	-0.051826	4.815640
246.614362	8000.322976	12.354023	-0.051824	4.815617
246.674813	8000.366722	12.359027	-0.051835	4.815629
246.581567	8000.333181	12.364032	-0.051818	4.815620
246.870877	8000.342222	12.369037	-0.051873	4.815621
246.746831	8000.343425	12.374042	-0.051850	4.815622
246.519034	8000.376042	12.379047	-0.051808	4.815633
246.734315	8000.375325	12.384051	-0.051848	4.815631
246.694335	8000.355474	12.389056	-0.051841	4.815626
246.590797	8000.320696	12.394061	-0.051822	4.815616
246.600954	8000.377505	12.399066	-0.051825	4.815633
246.736975	8000.372286	12.404071	-0.051850	4.815631
246.627798	8000.399368	12.409075	-0.051830	4.815639
246.904338	8000.359065	12.414080	-0.051882	4.815626
246.940976	8000.387468	12.419085	-0.051889	4.815634
246.884989	8000.329969	12.424090	-0.051879	4.815617
246.635655	8000.340870	12.429095	-0.051833	4.815622
246.803857	8000.392790	12.434099	-0.051865	4.815636
246.647073	8000.383844	12.439104	-0.051836	4.815634
246.841150	8000.393462	12.444109	-0.051872	4.815636
247.001934	8000.431375	12.449114	-0.051903	4.815646
246.925155	8000.416262	12.454119	-0.051889	4.815642
246.922789	8000.465389	12.459123	-0.051889	4.815657
246.726328	8000.467542	12.464128	-0.051852	4.815658
246.985646	8000.489979	12.469133	-0.051901	4.815664
246.910135	8000.471682	12.474138	-0.051887	4.815659
246.906205	8000.421444	12.479143	-0.051887	4.815644
246.919086	8000.433435	12.484147	-0.051890	4.815647
246.924636	8000.444238	12.489152	-0.051891	4.815651
246.929400	8000.469982	12.494157	-0.051892	4.815658
246.949702	8000.465004	12.499162	-0.051896	4.815656
246.878405	8000.373073	12.504167	-0.051883	4.815630
247.056727	8000.423023	12.509171	-0.051917	4.815644
246.831894	8000.447143	12.514176	-0.051875	4.815652
247.040574	8000.423888	12.519181	-0.051915	4.815644
246.959767	8000.451435	12.524186	-0.051900	4.815652
246.741181	8000.397681	12.529191	-0.051860	4.815638
246.883126	8000.428877	12.534195	-0.051886	4.815646
246.778297	8000.426122	12.539200	-0.051867	4.815646
246.832925	8000.389661	12.544205	-0.051878	4.815635
246.740150	8000.438376	12.549210	-0.051861	4.815650
246.993421	8000.452168	12.554215	-0.051908	4.815652
246.864731	8000.455431	12.559219	-0.051885	4.815654
246.805585	8000.424584	12.564224	-0.051874	4.815645
247.020436	8000.419589	12.569229	-0.051914	4.815643
246.885605	8000.463342	12.574234	-0.051890	4.815656
246.643617	8000.456203	12.579239	-0.051845	4.815655
246.754605	8000.439893	12.584243	-0.051866	4.815650
246.770233	8000.415612	12.589248	-0.051869	4.815643
246.696245	8000.388794	12.594253	-0.051856	4.815635
246.959579	8000.424115	12.599258	-0.051905	4.815644
247.084500	8000.379192	12.604263	-0.051929	4.815631
247.083377	8000.440090	12.609267	-0.051929	4.815648
246.920350	8000.440654	12.614272	-0.051899	4.815649
246.885048	8000.416606	12.619277	-0.051893	4.815642
246.992095	8000.455776	12.624282	-0.051913	4.815653
246.818589	8000.418783	12.629287	-0.051881	4.815643
246.863895	8000.455873	12.634291	-0.051890	4.815654
247.051089	8000.418379	12.639296	-0.051925	4.815642
246.986798	8000.405607	12.644301	-0.051913	4.815639
247.018638	8000.420045	12.649306	-0.051920	4.815643
247.064052	8000.321480	12.654311	-0.051928	4.815614
247.068075	8000.439074	12.659315	-0.051929	4.815648
246.910010	8000.473901	12.664320	-0.051900	4.815659
247.049961	8000.461270	12.669325	-0.051927	4.815655
246.968500	8000.436466	12.674330	-0.051912	4.815648
246.747304	8000.409373	12.679335	-0.051871	4.815641
246.789608	8000.465641	12.684339	-0.051879	4.815657
246.715437	8000.468729	12.689344	-0.051866	4.815658
246.915420	8000.407945	12.694349	-0.051903	4.815640
246.737794	8000.477701	12.699354	-0.051871	4.815661
246.799891	8000.402909	12.704359	-0.051883	4.815639
246.777717	8000.460257	12.709363	-0.051879	4.815656
246.654985	8000.437982	12.714368	-0.051856	4.815650
246.850544	8000.443352	12.719373	-0.051893	4.815650
246.924228	8000.463817	12.724378	-0.051907	4.815656
246.749112	8000.400093	12.729383	-0.051875	4.815638
247.076195	8000.448208	12.734387	-0.051936	4.815651
246.970778	8000.433693	12.739392	-0.051917	4.815647
247.013479	8000.421605	12.744397	-0.051925	4.815643
246.931138	8000.460877	12.749402	-0.051910	4.815655
247.181358	8000.395575	12.754407	-0.051957	4.815635
247.119635	8000.517435	12.759411	-0.051946	4.815670
246.939393	8000.481399	12.764416	-0.051913	4.815661
247.035565	8000.491550	12.769421	-0.051931	4.815663
247.177578	8000.496043	12.774426	-0.051958	4.815664
247.067603	8000.496408	12.779431	-0.051938	4.815665
247.053486	8000.557094	12.784435	-0.051935	4.815682
247.196311	8000.456919	12.789440	-0.051962	4.815652
247.076984	8000.494517	12.794445	-0.051940	4.815664
247.094977	8000.498046	12.799450	-0.051944	4.815665
247.255721	8000.443029	12.804455	-0.051974	4.815648
247.188967	8000.482556	12.809459	-0.051962	4.815660
247.040921	8000.432093	12.814464	-0.051935	4.815646
247.029195	8000.400954	12.819469	-0.051933	4.815637
247.177750	8000.460032	12.824474	-0.051961	4.815653
247.071177	8000.364317	12.829479	-0.051942	4.815626
247.012492	8000.433885	12.834483	-0.051931	4.815646
246.981834	8000.422732	12.839488	-0.051926	4.815643
246.882170	8000.381607	12.844493	-0.051908	4.815632
247.169167	8000.430134	12.849498	-0.051961	4.815645
247.057426	8000.426197	12.854503	-0.051941	4.815644
247.151704	8000.468363	12.859507	-0.051959	4.815656
247.032396	8000.410894	12.864512	-0.051937	4.815640
247.017205	8000.434175	12.869517	-0.051934	4.815646
247.079018	8000.485422	12.874522	-0.051946	4.815661
247.054404	8000.446595	12.879527	-0.051942	4.815650
246.946750	8000.450202	12.884531	-0.051922	4.815651
246.998458	8000.394467	12.889536	-0.051932	4.815635
246.945169	8000.322057	12.894541	-0.051923	4.815614
247.009767	8000.401122	12.899546	-0.051935	4.815637
246.972080	8000.362081	12.904551	-0.051928	4.815626
247.169967	8000.413421	12.909555	-0.051966	4.815640
246.929626	8000.414854	12.914560	-0.051921	4.815641
247.127068	8000.428801	12.919565	-0.051958	4.815644
247.027886	8000.481683	12.924570	-0.051940	4.815660
247.067379	8000.435361	12.929575	-0.051948	4.815646
246.963250	8000.457185	12.934579	-0.051929	4.815653
247.018133	8000.460251	12.939584	-0.051940	4.815654
246.815664	8000.464442	12.944589	-0.051902	4.815656
246.988121	8000.430980	12.949594	-0.051935	4.815646
246.990104	8000.412883	12.954599	-0.051935	4.815640
247.137050	8000.445230	12.959603	-0.051963	4.815649
247.181105	8000.353051	12.964608	-0.051972	4.815622
247.045341	8000.430970	12.969613	-0.051947	4.815645
247.203319	8000.477384	12.974618	-0.051976	4.815658
247.138216	8000.487030	12.979623	-0.051965	4.815661
247.063016	8000.439896	12.984627	-0.051951	4.815648
247.088943	8000.437147	12.989632	-0.051956	4.815647
247.111438	8000.404432	12.994637	-0.051961	4.815637
247.110682	8000.472814	12.999642	-0.051961	4.815657
247.046443	8000.407701	13.004647	-0.051949	4.815638
247.315129	8000.455929	13.009651	-0.052000	4.815651
247.219338	8000.393503	13.014656	-0.051982	4.815633
247.155986	8000.411723	13.019661	-0.051971	4.815639
247.069701	8000.425294	13.024666	-0.051955	4.815643
247.015114	8000.409476	13.029671	-0.051945	4.815639
247.120174	8000.432591	13.034675	-0.051965	4.815645
247.119938	8000.382413	13.039680	-0.051965	4.815631
247.156980	8000.415096	13.044685	-0.051973	4.815640
247.124200	8000.501111	13.049690	-0.051967	4.815665
247.033817	8000.480434	13.054695	-0.051950	4.815660
247.262522	8000.506643	13.059699	-0.051993	4.815666
247.148472	8000.451396	13.064704	-0.051972	4.815651
247.188886	8000.396543	13.069709	-0.051980	4.815634
247.176307	8000.429481	13.074714	-0.051978	4.815644
247.194379	8000.365716	13.079719	-0.051982	4.815625
247.317515	8000.381650	13.084723	-0.052005	4.815629
247.041984	8000.414553	13.089728	-0.051954	4.815640
247.007389	8000.405471	13.094733	-0.051948	4.815638
247.135802	8000.440719	13.099738	-0.051972	4.815647
246.933356	8000.356251	13.104743	-0.051935	4.815624
247.059347	8000.387186	13.109747	-0.051959	4.815632
247.342153	8000.360873	13.114752	-0.052012	4.815623
246.960933	8000.417680	13.119757	-0.051941	4.815641
247.162827	8000.371882	13.124762	-0.051979	4.815627
247.185102	8000.364800	13.129767	-0.051984	4.815625
247.143235	8000.404735	13.134771	-0.051976	4.815637
247.089457	8000.442339	13.139776	-0.051967	4.815648
247.124650	8000.449355	13.144781	-0.051973	4.815650
247.119541	8000.481347	13.149786	-0.051973	4.815659
246.926429	8000.409850	13.154791	-0.051937	4.815639
247.143765	8000.435873	13.159795	-0.051978	4.815646
246.905407	8000.431998	13.164800	-0.051934	4.815646
246.829489	8000.410489	13.169805	-0.051920	4.815640
247.131994	8000.459271	13.174810	-0.051977	4.815653
247.007825	8000.435903	13.179815	-0.051954	4.815646
247.121208	8000.453814	13.184819	-0.051976	4.815651
246.991361	8000.405785	13.189824	-0.051952	4.815638
246.969210	8000.411862	13.194829	-0.051948	4.815640
247.044237	8000.490030	13.199834	-0.051962	4.815662
246.928128	8000.409113	13.204839	-0.051941	4.815639
247.001135	8000.480839	13.209843	-0.051955	4.815660
247.200844	8000.445687	13.214848	-0.051992	4.815648
247.221629	8000.444990	13.219853	-0.051997	4.815648
247.243331	8000.481694	13.224858	-0.052001	4.815659
247.177449	8000.399463	13.229863	-0.051989	4.815635
247.291417	8000.407770	13.234867	-0.052011	4.815637
247.106979	8000.395165	13.239872	-0.051977	4.815634
247.165005	8000.368373	13.244877	-0.051988	4.815626
247.166053	8000.460284	13.249882	-0.051988	4.815653
246.964561	8000.454877	13.254887	-0.051951	4.815652
247.111245	8000.472265	13.259891	-0.051979	4.815656
246.994945	8000.475731	13.264896	-0.051958	4.815658
246.951627	8000.488938	13.269901	-0.051950	4.815662
246.935654	8000.481229	13.274906	-0.051947	4.815660
247.049771	8000.461766	13.279911	-0.051969	4.815654
247.261646	8000.468472	13.284915	-0.052009	4.815655
246.989947	8000.446960	13.289920	-0.051958	4.815650
247.005500	8000.391700	13.294925	-0.051962	4.815633
247.228720	8000.450933	13.299930	-0.052004	4.815650
246.992607	8000.396890	13.304935	-0.051960	4.815635
247.361500	8000.490556	13.309939	-0.052029	4.815660
247.323200	8000.484617	13.314944	-0.052022	4.815659
247.019593	8000.477537	13.319949	-0.051966	4.815658
247.163398	8000.523719	13.324954	-0.051993	4.815671
247.236371	8000.440558	13.329959	-0.052007	4.815646
247.273275	8000.505285	13.334963	-0.052014	4.815665
247.280808	8000.473393	13.339968	-0.052016	4.815656
247.409553	8000.428533	13.344973	-0.052040	4.815642
247.293520	8000.438412	13.349978	-0.052019	4.815646
247.291761	8000.464050	13.354983	-0.052019	4.815653
247.375800	8000.430207	13.359987	-0.052035	4.815643
247.197406	8000.442269	13.364992	-0.052002	4.815647
247.177047	8000.452647	13.369997	-0.051999	4.815650
247.263549	8000.516050	13.375002	-0.052015	4.815668
247.527777	8000.460592	13.380007	-0.052065	4.815651
247.533013	8000.463912	13.385011	-0.052066	4.815652
247.549344	8000.433233	13.390016	-0.052069	4.815643
247.441016	8000.434693	13.395021	-0.052050	4.815644
247.395875	8000.452143	13.400026	-0.052042	4.815649
247.423415	8000.415238	13.405031	-0.052047	4.815638
247.209016	8000.444869	13.410035	-0.052007	4.815648
247.310435	8000.438015	13.415040	-0.052027	4.815645
247.294473	8000.412148	13.420045	-0.052024	4.815638
247.393403	8000.427686	13.425050	-0.052043	4.815642
247.247752	8000.448829	13.430055	-0.052016	4.815649
247.330938	8000.479064	13.435059	-0.052032	4.815657
247.184067	8000.489506	13.440064	-0.052005	4.815661
247.143312	8000.451482	13.445069	-0.051998	4.815650
247.485573	8000.489166	13.450074	-0.052062	4.815659
247.350233	8000.423956	13.455079	-0.052037	4.815641
247.432891	8000.462727	13.460083	-0.052053	4.815652
247.243267	8000.457514	13.465088	-0.052018	4.815651
247.375302	8000.393480	13.470093	-0.052043	4.815632
247.264085	8000.449370	13.475098	-0.052022	4.815649
247.176000	8000.438344	13.480103	-0.052006	4.815646
247.336537	8000.486937	13.485107	-0.052036	4.815659
247.298843	8000.450031	13.490112	-0.052030	4.815649
247.345346	8000.414505	13.495117	-0.052039	4.815638
247.348269	8000.457311	13.500122	-0.052040	4.815651
247.438606	8000.390457	13.505127	-0.052057	4.815631
247.408434	8000.375039	13.510131	-0.052051	4.815626
247.469080	8000.400631	13.515136	-0.052063	4.815633
247.567766	8000.321096	13.520141	-0.052082	4.815610
247.453638	8000.392961	13.525146	-0.052061	4.815631
247.521555	8000.384491	13.530151	-0.052074	4.815628
247.580670	8000.473082	13.535155	-0.052085	4.815654
247.287834	8000.480063	13.540160	-0.052031	4.815657
247.494268	8000.439681	13.545165	-0.052070	4.815645
247.638923	8000.445286	13.550170	-0.052097	4.815646
247.665598	8000.453231	13.555175	-0.052102	4.815648
247.539445	8000.442649	13.560179	-0.052079	4.815645
247.561843	8000.452660	13.565184	-0.052084	4.815648
247.560350	8000.462279	13.570189	-0.052084	4.815651
247.637155	8000.466773	13.575194	-0.052099	4.815652
247.567938	8000.386623	13.580199	-0.052086	4.815629
247.762356	8000.403726	13.585203	-0.052123	4.815633
247.568548	8000.418739	13.590208	-0.052087	4.815638
247.598711	8000.395764	13.595213	-0.052093	4.815631
247.631184	8000.401667	13.600218	-0.052099	4.815633
247.407387	8000.354235	13.605223	-0.052058	4.815620
247.468074	8000.330691	13.610227	-0.052069	4.815613
247.313344	8000.370914	13.615232	-0.052041	4.815625
247.533629	8000.400190	13.620237	-0.052082	4.815633
247.679074	8000.367353	13.625242	-0.052110	4.815622
247.615587	8000.341775	13.630247	-0.052098	4.815615
247.805648	8000.353466	13.635251	-0.052134	4.815618
247.569364	8000.400897	13.640256	-0.052090	4.815633
247.637662	8000.350773	13.645261	-0.052103	4.815618
247.570007	8000.460787	13.650266	-0.052091	4.815650
247.545127	8000.385636	13.655271	-0.052087	4.815628
247.467154	8000.367298	13.660275	-0.052073	4.815623
247.495637	8000.435091	13.665280	-0.052078	4.815643
247.445013	8000.357382	13.670285	-0.052069	4.815621
247.518907	8000.482534	13.675290	-0.052083	4.815657
247.407398	8000.412372	13.680295	-0.052063	4.815637
247.452695	8000.376827	13.685299	-0.052072	4.815626
247.553437	8000.451145	13.690304	-0.052091	4.815647
247.625736	8000.373314	13.695309	-0.052105	4.815624
247.820981	8000.475886	13.700314	-0.052141	4.815653
247.610156	8000.420120	13.705319	-0.052102	4.815638
247.691268	8000.399047	13.710323	-0.052118	4.815631
247.612984	8000.402067	13.715328	-0.052104	4.815633
247.740323	8000.325138	13.720333	-0.052128	4.815610
247.654618	8000.397469	13.725338	-0.052112	4.815631
247.429901	8000.410908	13.730343	-0.052071	4.815636
247.571248	8000.418596	13.735347	-0.052097	4.815638
247.548351	8000.420387	13.740352	-0.052093	4.815638
247.485426	8000.414046	13.745357	-0.052082	4.815637
247.509347	8000.467878	13.750362	-0.052087	4.815652
247.547448	8000.385213	13.755367	-0.052094	4.815628
247.727177	8000.392462	13.760371	-0.052128	4.815629
247.721316	8000.399874	13.765376	-0.052127	4.815631
247.541063	8000.359563	13.770381	-0.052094	4.815621
247.629642	8000.428341	13.775386	-0.052111	4.815640
247.551451	8000.374749	13.780391	-0.052097	4.815625
247.628899	8000.315162	13.785395	-0.052111	4.815607
247.741040	8000.351212	13.790400	-0.052133	4.815617
247.762641	8000.349460	13.795405	-0.052137	4.815616
247.660500	8000.424726	13.800410	-0.052118	4.815639
247.459035	8000.434273	13.805415	-0.052081	4.815643
247.684469	8000.436930	13.810419	-0.052124	4.815642
247.597892	8000.421655	13.815424	-0.052108	4.815638
247.652441	8000.392670	13.820429	-0.052118	4.815630
247.476390	8000.401565	13.825434	-0.052086	4.815633
247.365072	8000.389089	13.830439	-0.052065	4.815630
247.678891	8000.409217	13.835443	-0.052124	4.815634
247.750906	8000.427519	13.840448	-0.052138	4.815639
247.746826	8000.390095	13.845453	-0.052138	4.815628
247.670170	8000.429461	13.850458	-0.052124	4.815640
247.676409	8000.438139	13.855463	-0.052125	4.815643
247.632050	8000.441715	13.860467	-0.052117	4.815644
247.655870	8000.457091	13.865472	-0.052122	4.815648
247.742495	8000.365608	13.870477	-0.052138	4.815621
247.881267	8000.427732	13.875482	-0.052165	4.815639
247.671875	8000.389080	13.880487	-0.052126	4.815628
247.746696	8000.354018	13.885491	-0.052140	4.815618
247.852213	8000.426278	13.890496	-0.052160	4.815638
247.727849	8000.361247	13.895501	-0.052137	4.815620
247.859997	8000.444626	13.900506	-0.052162	4.815644
247.632784	8000.370432	13.905511	-0.052120	4.815623
247.537210	8000.373169	13.910515	-0.052103	4.815624
247.518296	8000.434844	13.915520	-0.052100	4.815642
247.511140	8000.378143	13.920525	-0.052099	4.815626
247.715905	8000.455235	13.925530	-0.052137	4.815647
247.562567	8000.464502	13.930535	-0.052109	4.815651
247.678757	8000.399140	13.935539	-0.052131	4.815631
247.667904	8000.455607	13.940544	-0.052129	4.815648
247.709983	8000.396508	13.945549	-0.052138	4.815630
247.658940	8000.408520	13.950554	-0.052128	4.815634
247.405078	8000.433232	13.955559	-0.052082	4.815642
247.742242	8000.490061	13.960563	-0.052145	4.815657
247.592800	8000.441710	13.965568	-0.052117	4.815644
247.500979	8000.397508	13.970573	-0.052100	4.815631
247.609924	8000.388641	13.975578	-0.052121	4.815628
247.545412	8000.371592	13.980583	-0.052109	4.815624
247.456994	8000.433196	13.985587	-0.052093	4.815642
247.624452	8000.465881	13.990592	-0.052125	4.815651
247.397867	8000.421606	13.995597	-0.052083	4.815639
247.349713	8000.461439	14.000602	-0.052074	4.815651
247.460844	8000.412017	14.005607	-0.052095	4.815636
247.733313	8000.442150	14.010611	-0.052146	4.815643
247.622736	8000.457459	14.015616	-0.052126	4.815648
247.631874	8000.363638	14.020621	-0.052128	4.815621
247.911551	8000.467595	14.025626	-0.052181	4.815650
247.886870	8000.433038	14.030631	-0.052176	4.815640
247.708993	8000.402380	14.035635	-0.052144	4.815632
247.763819	8000.384081	14.040640	-0.052154	4.815626
247.829670	8000.359554	14.045645	-0.052167	4.815619
247.782777	8000.458158	14.050650	-0.052158	4.815648
247.602142	8000.399682	14.055655	-0.052125	4.815631
247.546590	8000.435120	14.060659	-0.052115	4.815642
247.521418	8000.443284	14.065664	-0.052111	4.815645
247.540257	8000.354963	14.070669	-0.052115	4.815619
247.779104	8000.455045	14.075674	-0.052160	4.815647
247.643629	8000.398377	14.080679	-0.052135	4.815631
247.530406	8000.391211	14.085683	-0.052114	4.815629
247.392547	8000.446664	14.090688	-0.052089	4.815646
247.535233	8000.363578	14.095693	-0.052115	4.815621
247.723041	8000.435051	14.100698	-0.052151	4.815641
247.618134	8000.402384	14.105703	-0.052132	4.815632
247.733400	8000.406440	14.110707	-0.052153	4.815633
247.698954	8000.399496	14.115712	-0.052147	4.815631
247.581199	8000.377301	14.120717	-0.052126	4.815625
247.795766	8000.453486	14.125722	-0.052166	4.815646
247.559107	8000.458183	14.130727	-0.052122	4.815649
247.666847	8000.434342	14.135731	-0.052143	4.815641
247.746631	8000.448499	14.140736	-0.052158	4.815645
247.720546	8000.403237	14.145741	-0.052153	4.815632
247.654279	8000.453455	14.150746	-0.052141	4.815647
247.723543	8000.367028	14.155751	-0.052155	4.815621
247.649825	8000.412851	14.160755	-0.052141	4.815635
247.756565	8000.442404	14.165760	-0.052162	4.815643
247.449175	8000.393600	14.170765	-0.052105	4.815630
247.873279	8000.446514	14.175770	-0.052184	4.815644
247.761003	8000.385953	14.180775	-0.052163	4.815626
247.726052	8000.366183	14.185779	-0.052157	4.815621
247.702026	8000.428843	14.190784	-0.052153	4.815639
247.941909	8000.375123	14.195789	-0.052198	4.815622
248.013131	8000.477800	14.200794	-0.052212	4.815652
247.635129	8000.401133	14.205799	-0.052142	4.815631
247.757528	8000.425602	14.210803	-0.052165	4.815638
247.658990	8000.444313	14.215808	-0.052147	4.815644
247.560732	7999.335048	14.220813	-0.052128	4.815320

247.595691	7996.182840	14.225818	-0.052133	4.814399
247.639377	7990.612101	14.230823	-0.052138	4.812770
247.571166	7983.919862	14.235827	-0.052121	4.810812
247.536067	7976.674095	14.240832	-0.052110	4.808692
247.358895	7968.979401	14.245837	-0.052072	4.806440
247.473594	7961.203378	14.250842	-0.052089	4.804162
247.467104	7953.306671	14.255847	-0.052083	4.801848
247.605187	7945.361662	14.260851	-0.052104	4.799518
247.469084	7937.452570	14.265856	-0.052074	4.797199
247.330443	7929.393107	14.270861	-0.052043	4.794834
247.485959	7921.445055	14.275866	-0.052067	4.792500
247.396437	7913.348570	14.280871	-0.052046	4.790122
247.478605	7905.421053	14.285875	-0.052056	4.787792
247.307000	7897.370714	14.290880	-0.052019	4.785425
247.312820	7889.422347	14.295885	-0.052016	4.783087
247.365227	7881.472140	14.300890	-0.052020	4.780747
247.175693	7873.379504	14.305895	-0.051980	4.778364
247.188107	7865.433472	14.310899	-0.051978	4.776023
247.015233	7857.364000	14.315904	-0.051941	4.773645
246.993773	7849.365109	14.320909	-0.051932	4.771286
246.950068	7841.397413	14.325914	-0.051919	4.768935
246.795392	7833.360406	14.330919	-0.051885	4.766563
246.935755	7825.340563	14.335923	-0.051906	4.764194
246.594132	7817.415016	14.340928	-0.051838	4.761853
246.898253	7809.344859	14.345933	-0.051890	4.759466
246.960000	7801.390850	14.350938	-0.051896	4.757113
246.658466	7793.343820	14.355943	-0.051835	4.754732
246.759612	7785.323367	14.360947	-0.051849	4.752357
246.791893	7777.307189	14.365952	-0.051850	4.749982
246.703016	7769.341096	14.370957	-0.051829	4.747621
246.700093	7761.315714	14.375962	-0.051823	4.745241
246.816520	7753.382925	14.380967	-0.051840	4.742887
246.424039	7745.332126	14.385971	-0.051762	4.740499
246.400639	7737.363858	14.390976	-0.051753	4.738132
246.434056	7729.315064	14.395981	-0.051754	4.735740
246.418351	7721.326551	14.400986	-0.051747	4.733365
246.276909	7713.281061	14.405991	-0.051715	4.730973
246.373616	7705.309030	14.410995	-0.051729	4.728600
246.357030	7697.294869	14.416000	-0.051721	4.726214
246.195919	7689.240532	14.421005	-0.051686	4.723815
246.015312	7681.336797	14.426010	-0.051647	4.721460
245.964881	7673.314677	14.431015	-0.051633	4.719068
246.021110	7665.387503	14.436019	-0.051639	4.716702
245.872682	7657.317295	14.441024	-0.051606	4.714294
245.797621	7649.243496	14.446029	-0.051587	4.711883
246.103113	7641.290649	14.451034	-0.051639	4.709506
245.843636	7633.248729	14.456039	-0.051586	4.707102
245.706407	7625.287049	14.461043	-0.051556	4.704721
245.773227	7617.388274	14.466048	-0.051563	4.702357
245.587336	7609.272795	14.471053	-0.051524	4.699927
245.687023	7601.332297	14.476058	-0.051537	4.697548
245.722019	7593.289150	14.481063	-0.051539	4.695137
245.594616	7585.296978	14.486067	-0.051510	4.692741
245.436641	7577.259864	14.491072	-0.051476	4.690330
245.168160	7569.275161	14.496077	-0.051421	4.687933
245.621059	7561.295688	14.501082	-0.051501	4.685536
245.388197	7553.284118	14.506087	-0.051453	4.683129
245.489331	7545.267139	14.511091	-0.051467	4.680718
245.521541	7537.308895	14.516096	-0.051468	4.678325
245.499747	7529.255929	14.521101	-0.051459	4.675901
245.486112	7521.267312	14.526106	-0.051451	4.673495
245.456952	7513.178114	14.531111	-0.051441	4.671058
245.239036	7505.215546	14.536115	-0.051396	4.668658
245.107060	7497.227513	14.541120	-0.051366	4.666250
244.927957	7489.231061	14.546125	-0.051328	4.663837
245.102699	7481.269123	14.551130	-0.051356	4.661433
244.759338	7473.211191	14.556135	-0.051287	4.658999
244.780117	7465.240446	14.561139	-0.051286	4.656590
244.930029	7457.201989	14.566144	-0.051309	4.654160
244.737500	7449.179019	14.571149	-0.051268	4.651733
244.657284	7441.193635	14.576154	-0.051248	4.649316
244.610786	7433.230052	14.581159	-0.051235	4.646904
244.804887	7425.223838	14.586163	-0.051266	4.644478
244.831117	7417.274896	14.591168	-0.051266	4.642068
244.624789	7409.152610	14.596173	-0.051223	4.639604
244.826798	7401.237069	14.601178	-0.051256	4.637202
244.714623	7393.235600	14.606183	-0.051230	4.634772
244.469649	7385.234071	14.611187	-0.051179	4.632341
244.721885	7377.167667	14.616192	-0.051221	4.629889
244.658041	7369.197461	14.621197	-0.051205	4.627466
244.667275	7361.149472	14.626202	-0.051201	4.625017
244.442456	7353.197848	14.631207	-0.051155	4.622596
244.501666	7345.190180	14.636211	-0.051161	4.620157
244.379473	7337.214315	14.641216	-0.051133	4.617726
244.182073	7329.205847	14.646221	-0.051092	4.615284
244.349032	7321.177129	14.651226	-0.051118	4.612834
244.263563	7313.112805	14.656231	-0.051097	4.610373
244.091969	7305.186740	14.661235	-0.051060	4.607952
244.299933	7297.149256	14.666240	-0.051094	4.605496
244.178321	7289.141781	14.671245	-0.051067	4.603047
244.074034	7281.184517	14.676250	-0.051042	4.600613
243.957672	7273.174420	14.681255	-0.051016	4.598161
243.948652	7265.191940	14.686259	-0.051009	4.595717
243.981317	7257.186146	14.691264	-0.051010	4.593264
243.827219	7249.096385	14.696269	-0.050977	4.590784
243.811139	7241.140019	14.701274	-0.050969	4.588343
243.735258	7233.098532	14.706279	-0.050950	4.585875
243.682659	7225.141657	14.711283	-0.050935	4.583432
243.558525	7217.136410	14.716288	-0.050907	4.580973
243.511267	7209.128197	14.721293	-0.050894	4.578511
243.586590	7201.135116	14.726298	-0.050903	4.576053
243.555491	7193.128389	14.731303	-0.050892	4.573589
243.569119	7185.097461	14.736307	-0.050890	4.571116
243.225741	7177.126859	14.741312	-0.050821	4.568660
243.254665	7169.089420	14.746317	-0.050821	4.566183
243.444553	7161.148818	14.751322	-0.050852	4.563735
243.588931	7153.156965	14.756327	-0.050874	4.561269
243.504850	7145.138019	14.761331	-0.050853	4.558793
243.427687	7137.133543	14.766336	-0.050834	4.556320
243.354869	7129.100104	14.771341	-0.050816	4.553837
243.259682	7121.132760	14.776346	-0.050793	4.551374
243.073446	7113.115766	14.781351	-0.050754	4.548893
243.086618	7105.110236	14.786355	-0.050751	4.546415
243.199247	7097.102484	14.791360	-0.050767	4.543934
242.903718	7089.143681	14.796365	-0.050707	4.541467
242.887264	7081.076966	14.801370	-0.050700	4.538966
242.851370	7073.130522	14.806375	-0.050688	4.536501
242.795424	7065.097047	14.811379	-0.050673	4.534007
242.782658	7057.106934	14.816384	-0.050665	4.531525
242.720483	7049.034161	14.821389	-0.050649	4.529016
242.488452	7041.159783	14.826394	-0.050601	4.526567
242.370391	7033.103362	14.831399	-0.050574	4.524061
242.477861	7025.125032	14.836403	-0.050589	4.521578
242.545860	7017.136311	14.841408	-0.050597	4.519090
242.580895	7009.149217	14.846413	-0.050599	4.516601
242.634593	7001.092298	14.851418	-0.050604	4.514089
242.344492	6993.004583	14.856423	-0.050545	4.511565
242.485678	6985.048968	14.861427	-0.050566	4.509082
242.510219	6977.073682	14.866432	-0.050566	4.506591
242.235241	6969.029465	14.871437	-0.050510	4.504077
242.230336	6961.091302	14.876442	-0.050504	4.501595
241.996212	6953.043851	14.881447	-0.050456	4.499077
241.975350	6945.098764	14.886451	-0.050447	4.496590
242.007697	6937.108757	14.891456	-0.050448	4.494087
241.789042	6929.027985	14.896461	-0.050402	4.491554
241.754555	6921.038664	14.901466	-0.050391	4.489049
241.781292	6913.042271	14.906471	-0.050391	4.486541
241.733433	6905.026246	14.911475	-0.050378	4.484024
241.756712	6897.089538	14.916480	-0.050377	4.481532
241.742132	6889.041437	14.921485	-0.050369	4.479003
241.743565	6881.089047	14.926490	-0.050365	4.476502
241.606931	6873.047372	14.931495	-0.050335	4.473972
241.694796	6865.018723	14.936499	-0.050346	4.471445
241.749492	6857.043517	14.941504	-0.050351	4.468933
241.621460	6849.006542	14.946509	-0.050323	4.466400
241.637809	6841.028919	14.951514	-0.050321	4.463885
241.664094	6833.026986	14.956519	-0.050321	4.461360
241.508378	6825.003103	14.961523	-0.050287	4.458827
241.390042	6817.032799	14.966528	-0.050260	4.456309
241.227705	6808.991558	14.971533	-0.050225	4.453767
241.311419	6801.018984	14.976538	-0.050236	4.451246
241.125680	6793.009970	14.981543	-0.050196	4.448712
241.264608	6785.003341	14.986547	-0.050217	4.446177
241.302369	6777.045922	14.991552	-0.050219	4.443657
241.154243	6769.031496	14.996557	-0.050187	4.441116
241.323578	6761.012478	15.001562	-0.050214	4.438574
241.108882	6753.027889	15.006567	-0.050169	4.436040
241.162016	6744.982271	15.011571	-0.050174	4.433486
241.060789	6736.959188	15.016576	-0.050150	4.430936
241.008440	6728.945958	15.021581	-0.050135	4.428389
241.047025	6720.985109	15.026586	-0.050138	4.425858
240.973332	6712.992214	15.031591	-0.050119	4.423314
240.914614	6704.972363	15.036595	-0.050103	4.420760
240.903219	6696.994665	15.041600	-0.050096	4.418218
240.945004	6688.958091	15.046605	-0.050099	4.415657
240.731126	6680.986902	15.051610	-0.050055	4.413113
240.444597	6672.926683	15.056615	-0.049996	4.410539
240.598233	6664.984492	15.061619	-0.050020	4.408004
240.404804	6656.956688	15.066624	-0.049979	4.405438
240.352877	6648.980147	15.071629	-0.049965	4.402888
240.556913	6641.002075	15.076634	-0.049998	4.400337
240.427795	6633.005846	15.081639	-0.049969	4.397777
240.366006	6625.002474	15.086643	-0.049952	4.395213
240.385269	6616.985859	15.091648	-0.049951	4.392644
240.284729	6608.931229	15.096653	-0.049928	4.390061
240.574689	6600.992270	15.101658	-0.049977	4.387516
240.407614	6592.927830	15.106663	-0.049941	4.384926
240.328000	6585.009503	15.111667	-0.049921	4.382382
240.173981	6577.009755	15.116672	-0.049888	4.379810
240.251288	6569.033844	15.121677	-0.049897	4.377246
240.105316	6561.002685	15.126682	-0.049865	4.374661
240.012547	6552.995704	15.131687	-0.049843	4.372083
239.918817	6544.926661	15.136691	-0.049820	4.369483
240.100966	6536.996640	15.141696	-0.049850	4.366928
239.928189	6528.936740	15.146701	-0.049813	4.364327
239.837078	6521.047442	15.151706	-0.049791	4.361780
239.697598	6512.987835	15.156711	-0.049760	4.359177
239.817938	6505.022621	15.161715	-0.049777	4.356604
239.737562	6496.992719	15.166720	-0.049758	4.354007
239.557043	6488.877048	15.171725	-0.049719	4.351381
239.776623	6480.903794	15.176730	-0.049755	4.348801
239.781044	6472.913601	15.181735	-0.049751	4.346214
239.551143	6464.894520	15.186739	-0.049703	4.343613
239.692493	6456.966877	15.191744	-0.049725	4.341044
239.434641	6448.969604	15.196749	-0.049672	4.338447
239.470107	6441.001726	15.201754	-0.049674	4.335860
239.307417	6432.934301	15.206759	-0.049638	4.333239
239.301740	6424.917386	15.211763	-0.049633	4.330633
239.203888	6416.955308	15.216768	-0.049609	4.328042
239.100060	6408.919535	15.221773	-0.049585	4.325426
239.207744	6400.984586	15.226778	-0.049600	4.322843
239.056313	6392.941405	15.231783	-0.049567	4.320221
238.850042	6384.967601	15.236787	-0.049524	4.317620
239.011695	6376.965387	15.241792	-0.049549	4.315011
239.049395	6368.943094	15.246797	-0.049552	4.312392
239.092839	6360.918842	15.251802	-0.049555	4.309772
238.917963	6352.912230	15.256807	-0.049517	4.307154
238.876634	6344.909308	15.261811	-0.049505	4.304536
238.859302	6336.973655	15.266816	-0.049497	4.301939
238.742671	6328.927954	15.271821	-0.049470	4.299304
238.797418	6320.975485	15.276826	-0.049475	4.296699
238.808573	6312.925118	15.281831	-0.049473	4.294060
238.563470	6304.907905	15.286835	-0.049422	4.291428
238.524092	6296.916277	15.291840	-0.049410	4.288805
238.484709	6288.896301	15.296845	-0.049398	4.286170
238.442587	6280.932632	15.301850	-0.049385	4.283553
238.368166	6272.960440	15.306855	-0.049366	4.280931
238.387162	6264.937658	15.311859	-0.049365	4.278291
238.419724	6256.961185	15.316864	-0.049366	4.275665
238.198995	6248.873987	15.321869	-0.049320	4.272999
238.252000	6240.872808	15.326874	-0.049325	4.270362
238.285555	6232.904510	15.331879	-0.049326	4.267734
238.159376	6224.854585	15.336883	-0.049298	4.265076
238.128586	6216.931921	15.341888	-0.049288	4.262459
238.195883	6208.851890	15.346893	-0.049295	4.259789
238.176251	6200.959536	15.351898	-0.049287	4.257179
238.034791	6192.882006	15.356903	-0.049255	4.254505
238.004356	6184.880085	15.361907	-0.049245	4.251856
238.017227	6176.885738	15.366912	-0.049242	4.249207
237.816969	6168.907982	15.371917	-0.049200	4.246561
237.962291	6160.901100	15.376922	-0.049222	4.243906
237.875660	6152.959344	15.381927	-0.049202	4.241269
237.793880	6144.881476	15.386931	-0.049181	4.238585
237.651848	6136.952299	15.391936	-0.049150	4.235949
237.660076	6128.914911	15.396941	-0.049147	4.233276
237.481757	6120.903978	15.401946	-0.049109	4.230609
237.600406	6112.890412	15.406951	-0.049126	4.227942
237.751997	6104.895877	15.411955	-0.049149	4.225279
237.818117	6096.920097	15.416960	-0.049157	4.222621
237.546641	6088.930407	15.421965	-0.049101	4.219953
237.434060	6080.977571	15.426970	-0.049075	4.217297
237.443369	6072.968177	15.431975	-0.049072	4.214622
237.478749	6064.912655	15.436979	-0.049074	4.211930
237.453243	6056.932263	15.441984	-0.049064	4.209260
237.465360	6048.928745	15.446989	-0.049062	4.206582
237.309743	6040.958833	15.451994	-0.049028	4.203912
237.157864	6032.991145	15.456999	-0.048995	4.201240
237.134220	6024.942654	15.462003	-0.048986	4.198541
237.210040	6016.965044	15.467008	-0.048995	4.195865
236.985454	6008.857042	15.472013	-0.048948	4.193141
237.009734	6000.806824	15.477018	-0.048948	4.190436
236.957984	5992.869157	15.482023	-0.048933	4.187767
236.897090	5984.849661	15.487027	-0.048917	4.185069
236.999459	5976.958928	15.492032	-0.048931	4.182414
236.856188	5968.859768	15.497037	-0.048900	4.179684
236.962466	5960.937375	15.502042	-0.048915	4.177015
236.887206	5952.913133	15.507047	-0.048896	4.174308
236.809274	5944.881276	15.512051	-0.048876	4.171597
237.015786	5936.929235	15.517056	-0.048910	4.168914
236.820267	5928.884975	15.522061	-0.048869	4.166193
236.645248	5920.911816	15.527066	-0.048831	4.163495
236.666656	5912.933507	15.532071	-0.048830	4.160796
236.557669	5904.934432	15.537075	-0.048805	4.158086
236.396304	5896.907426	15.542080	-0.048770	4.155365
236.301318	5888.867798	15.547085	-0.048748	4.152638
236.338860	5880.883146	15.552090	-0.048750	4.149930
236.144151	5872.884272	15.557095	-0.048709	4.147212
236.239263	5864.881415	15.562099	-0.048722	4.144495
236.436372	5856.943506	15.567104	-0.048753	4.141799
236.146129	5848.859256	15.572109	-0.048694	4.139046
236.263052	5840.934617	15.577114	-0.048711	4.136350
236.216664	5832.887209	15.582119	-0.048698	4.133608
236.129625	5824.837484	15.587123	-0.048677	4.130864
236.074760	5816.884404	15.592128	-0.048662	4.128151
235.891084	5808.884604	15.597133	-0.048623	4.125418
235.993946	5800.935375	15.602138	-0.048637	4.122705
235.850422	5792.893615	15.607143	-0.048605	4.119955
235.682404	5784.948558	15.612147	-0.048569	4.117236
235.843305	5776.921722	15.617152	-0.048594	4.114492
235.582369	5768.869570	15.622157	-0.048541	4.111731
235.578135	5760.889743	15.627162	-0.048535	4.108997
235.662768	5752.879088	15.632167	-0.048546	4.106252
235.458248	5744.853884	15.637171	-0.048503	4.103495
235.618088	5736.905619	15.642176	-0.048528	4.100769
235.553926	5728.884018	15.647181	-0.048511	4.098012
235.549348	5720.920005	15.652186	-0.048505	4.095274
235.433426	5712.881298	15.657191	-0.048479	4.092507
235.278455	5704.861398	15.662195	-0.048445	4.089744
235.348735	5696.946836	15.667200	-0.048453	4.087018
235.487920	5688.881800	15.672205	-0.048474	4.084240
235.370438	5680.974449	15.677210	-0.048448	4.081511
235.366019	5672.957620	15.682215	-0.048442	4.078744
235.282549	5664.958450	15.687219	-0.048422	4.075979
235.132057	5656.953907	15.692224	-0.048389	4.073210
234.887186	5648.892835	15.697229	-0.048338	4.070419
235.085401	5640.931163	15.702234	-0.048370	4.067666
235.025145	5632.924110	15.707239	-0.048354	4.064892
234.979215	5624.948079	15.712243	-0.048341	4.062126
235.037468	5616.944407	15.717248	-0.048347	4.059351
234.886629	5608.956665	15.722253	-0.048314	4.056577
234.752725	5600.965665	15.727258	-0.048284	4.053799
234.520323	5592.934941	15.732263	-0.048236	4.051005
234.667037	5584.911856	15.737267	-0.048258	4.048217
234.665166	5576.922942	15.742272	-0.048253	4.045436
234.593018	5568.945202	15.747277	-0.048235	4.042657
234.771590	5560.966766	15.752282	-0.048263	4.039879
234.550891	5552.998332	15.757287	-0.048217	4.037096
234.292564	5544.949474	15.762291	-0.048164	4.034283
234.456426	5536.817494	15.767296	-0.048190	4.031446
234.295569	5528.840121	15.772301	-0.048155	4.028655
234.197842	5520.895043	15.777306	-0.048132	4.025875
234.068526	5512.910514	15.782311	-0.048103	4.023079
234.299489	5504.911283	15.787315	-0.048141	4.020281
234.094778	5496.948368	15.792320	-0.048098	4.017487
233.823793	5488.863216	15.797325	-0.048043	4.014647
234.098960	5480.914276	15.802330	-0.048089	4.011862
234.137620	5472.902253	15.807335	-0.048092	4.009049
233.897541	5464.909271	15.812339	-0.048042	4.006236
233.798697	5456.916517	15.817344	-0.048019	4.003423
233.795656	5448.925081	15.822349	-0.048013	4.000610
233.666280	5440.950346	15.827354	-0.047984	3.997800
233.737527	5432.924283	15.832359	-0.047993	3.994972
233.930313	5424.874403	15.837363	-0.048024	3.992136
233.818785	5416.875159	15.842368	-0.047998	3.989311
233.646779	5408.887088	15.847373	-0.047961	3.986487
233.842062	5400.924751	15.852378	-0.047993	3.983676
233.785743	5392.900303	15.857383	-0.047977	3.980837
233.505944	5384.930890	15.862387	-0.047920	3.978011
233.569204	5376.956388	15.867392	-0.047927	3.975188
233.535555	5368.929603	15.872397	-0.047916	3.972342
233.526249	5360.909194	15.877402	-0.047910	3.969497
233.478462	5352.947374	15.882407	-0.047896	3.966670
233.434845	5344.939220	15.887411	-0.047883	3.963825
233.478267	5337.003770	15.892416	-0.047886	3.961004
233.268310	5328.982668	15.897421	-0.047842	3.958147
233.090222	5321.010617	15.902426	-0.047804	3.955306
233.138754	5312.947498	15.907431	-0.047808	3.952435
232.832704	5304.903170	15.912435	-0.047746	3.949562
232.880416	5296.962072	15.917440	-0.047750	3.946729
232.821956	5288.920876	15.922445	-0.047735	3.943857
232.918581	5280.964376	15.927450	-0.047748	3.941016
232.979746	5272.997010	15.932455	-0.047754	3.938169
233.003807	5264.971817	15.937459	-0.047754	3.935298
232.910627	5256.977516	15.942464	-0.047732	3.932434
232.634608	5248.946008	15.947469	-0.047675	3.929551
232.778625	5241.012487	15.952474	-0.047697	3.926709
232.749964	5232.982942	15.957479	-0.047687	3.923827
232.725489	5225.014721	15.962483	-0.047678	3.920965
232.766124	5217.022094	15.967488	-0.047681	3.918093
232.780044	5209.020196	15.972493	-0.047678	3.915216
232.824283	5201.000945	15.977498	-0.047682	3.912330
232.406646	5192.988884	15.982503	-0.047599	3.909437
232.638193	5184.987437	15.987507	-0.047637	3.906557
232.718245	5177.005723	15.992512	-0.047647	3.903679
232.270311	5168.982181	15.997517	-0.047559	3.900775
232.329961	5161.013408	16.002522	-0.047565	3.897897
232.442844	5153.007993	16.007527	-0.047581	3.895005
232.244583	5144.961052	16.012531	-0.047540	3.892090
232.261925	5136.954507	16.017536	-0.047538	3.889192
232.078525	5128.995597	16.022541	-0.047499	3.886305
232.192615	5121.004452	16.027546	-0.047515	3.883409
231.946431	5113.011835	16.032551	-0.047465	3.880504
231.837633	5105.063487	16.037555	-0.047440	3.877616
231.951872	5097.022361	16.042560	-0.047456	3.874696
231.798686	5088.746865	16.047565	-0.047422	3.871683
231.711055	5080.843873	16.052570	-0.047401	3.868805
231.765077	5072.903962	16.057575	-0.047406	3.865914
231.676353	5064.953803	16.062579	-0.047385	3.863014
231.522071	5056.984166	16.067584	-0.047351	3.860104
231.637328	5048.966451	16.072589	-0.047368	3.857179
231.661127	5040.978619	16.077594	-0.047368	3.854261
231.652801	5032.962762	16.082599	-0.047361	3.851330
231.318605	5024.988202	16.087603	-0.047294	3.848406
231.693171	5017.023756	16.092608	-0.047359	3.845497
231.514471	5009.016972	16.097613	-0.047321	3.842559
231.477772	5001.045854	16.102618	-0.047309	3.839635
231.383046	4993.081551	16.107623	-0.047287	3.836710
231.180945	4985.053827	16.112627	-0.047244	3.833757
231.121077	4977.055716	16.117632	-0.047228	3.830816
231.077010	4969.034036	16.122637	-0.047215	3.827864
231.212217	4961.012557	16.127642	-0.047235	3.824914
231.076550	4953.076280	16.132647	-0.047205	3.821987
230.808962	4945.038635	16.137651	-0.047151	3.819018
231.121133	4937.093969	16.142656	-0.047204	3.816093
230.767949	4929.080583	16.147661	-0.047133	3.813126
230.638372	4921.073257	16.152666	-0.047104	3.810164
230.885789	4913.066260	16.157671	-0.047145	3.807207
230.878269	4905.066812	16.162675	-0.047139	3.804246
230.752267	4897.138687	16.167680	-0.047111	3.801306
230.420356	4889.125347	16.172685	-0.047044	3.798328
230.643105	4881.122666	16.177690	-0.047081	3.795364
230.653517	4873.074864	16.182695	-0.047078	3.792376
230.319817	4865.026167	16.187699	-0.047011	3.789378
230.473029	4857.107646	16.192704	-0.047035	3.786436
230.257062	4849.044603	16.197709	-0.046989	3.783430
230.161514	4841.105664	16.202714	-0.046967	3.780471
230.146321	4833.097825	16.207719	-0.046959	3.777485
230.005794	4825.105581	16.212723	-0.046928	3.774500
230.053478	4817.120011	16.217728	-0.046932	3.771520
229.948096	4809.079066	16.222733	-0.046908	3.768513
230.158666	4801.090393	16.227738	-0.046942	3.765530
229.806898	4793.114049	16.232743	-0.046872	3.762536
229.698923	4785.117572	16.237747	-0.046847	3.759539
229.942787	4777.152463	16.242752	-0.046887	3.756558
229.833464	4769.107271	16.247757	-0.046862	3.753538
229.712684	4761.094254	16.252762	-0.046835	3.750526
229.717853	4753.099827	16.257767	-0.046831	3.747522
229.724266	4745.079375	16.262771	-0.046827	3.744506
229.773882	4737.163009	16.267776	-0.046831	3.741528
229.529544	4729.137173	16.272781	-0.046781	3.738499
229.631074	4721.134250	16.277786	-0.046795	3.735484
229.654851	4713.137699	16.282791	-0.046795	3.732468
229.311429	4705.134510	16.287795	-0.046726	3.729437
229.322624	4697.177376	16.292800	-0.046723	3.726431
229.433804	4689.127054	16.297805	-0.046739	3.723388
229.417095	4681.148331	16.302810	-0.046731	3.720368
229.193601	4673.222314	16.307815	-0.046684	3.717360
229.197799	4665.191044	16.312819	-0.046680	3.714315
229.253583	4657.069279	16.317824	-0.046686	3.711234
229.187905	4649.091932	16.322829	-0.046669	3.708203
229.317891	4641.110084	16.327834	-0.046688	3.705173
229.493608	4633.153888	16.332839	-0.046716	3.702151
229.304845	4625.185290	16.337843	-0.046676	3.699112
229.182693	4617.257461	16.342848	-0.046648	3.696089
229.074737	4609.218219	16.347853	-0.046623	3.693020
228.971388	4601.195220	16.352858	-0.046599	3.689956
228.616081	4593.249506	16.357863	-0.046528	3.686912
228.627763	4585.198036	16.362867	-0.046525	3.683834
228.622493	4577.259637	16.367872	-0.046520	3.680797
228.530356	4569.266762	16.372877	-0.046498	3.677734
228.490020	4561.256773	16.377882	-0.046485	3.674663
228.634372	4553.212645	16.382887	-0.046507	3.671581
228.496496	4545.211258	16.387891	-0.046477	3.668506
228.626005	4537.238417	16.392896	-0.046496	3.665446
228.669996	4529.230082	16.397901	-0.046499	3.662368
228.651140	4521.228675	16.402906	-0.046491	3.659288
228.574890	4513.284910	16.407911	-0.046472	3.656226
228.477033	4505.249744	16.412915	-0.046449	3.653126
228.419654	4497.236473	16.417920	-0.046433	3.650033
228.245367	4489.241276	16.422925	-0.046396	3.646941
228.305634	4481.238425	16.427930	-0.046402	3.643849
228.482910	4473.278644	16.432935	-0.046430	3.640775
228.140539	4465.319539	16.437939	-0.046362	3.637685
228.095707	4457.321752	16.442944	-0.046349	3.634585
227.858360	4449.289485	16.447949	-0.046299	3.631463
227.873467	4441.269943	16.452954	-0.046297	3.628351
227.875812	4433.251747	16.457959	-0.046293	3.625236
227.810960	4425.292513	16.462963	-0.046276	3.622140
227.899533	4417.294044	16.467968	-0.046288	3.619030
227.781629	4409.320182	16.472973	-0.046261	3.615921
227.787496	4401.313263	16.477978	-0.046257	3.612800
227.659572	4393.297957	16.482983	-0.046228	3.609669
227.641704	4385.320999	16.487987	-0.046220	3.606553
227.775462	4377.354510	16.492992	-0.046240	3.603444
227.589101	4369.365873	16.497997	-0.046201	3.600313
227.530026	4361.410218	16.503002	-0.046185	3.597197
227.382031	4353.381076	16.508007	-0.046152	3.594047
227.245350	4345.352661	16.513011	-0.046122	3.590894
227.217113	4337.381559	16.518016	-0.046112	3.587764
227.111512	4329.372996	16.523021	-0.046087	3.584615
227.108510	4321.407717	16.528026	-0.046082	3.581482
227.335043	4313.401772	16.533031	-0.046119	3.578338
227.171141	4305.418606	16.538035	-0.046084	3.575189
227.169106	4297.416454	16.543040	-0.046079	3.572033
227.000706	4289.386146	16.548045	-0.046042	3.568860
227.157310	4281.381801	16.553050	-0.046067	3.565703
227.099284	4273.433474	16.558055	-0.046051	3.562559
227.126993	4265.399097	16.563059	-0.046051	3.559381
227.008043	4257.499387	16.568064	-0.046024	3.556249
226.906475	4249.386543	16.573069	-0.046001	3.553030
226.943229	4241.335282	16.578074	-0.046003	3.549837
226.899904	4233.386041	16.583079	-0.045990	3.546679
227.020939	4225.401747	16.588083	-0.046007	3.543509
226.842753	4217.450174	16.593088	-0.045969	3.540340
226.506702	4209.466759	16.598093	-0.045902	3.537152
226.590203	4201.465269	16.603098	-0.045913	3.533965
226.488880	4193.439586	16.608103	-0.045889	3.530761
226.582976	4185.427505	16.613107	-0.045901	3.527565
226.582814	4177.466524	16.618112	-0.045897	3.524384
226.585476	4169.477412	16.623117	-0.045892	3.521188
226.297282	4161.518588	16.628122	-0.045834	3.517993
226.324714	4153.510992	16.633127	-0.045834	3.514785
225.995788	4145.490642	16.638131	-0.045768	3.511558
226.271940	4137.484806	16.643136	-0.045814	3.508353
226.277424	4129.475243	16.648141	-0.045811	3.505135
226.126851	4121.516166	16.653146	-0.045778	3.501929
226.043546	4113.552248	16.658151	-0.045757	3.498721
225.824052	4105.561363	16.663155	-0.045712	3.495494
226.073138	4097.563823	16.668160	-0.045753	3.492277
225.894610	4089.552893	16.673165	-0.045715	3.489037
225.820627	4081.575270	16.678170	-0.045696	3.485812
225.670442	4073.610291	16.683175	-0.045663	3.482586
225.776762	4065.578582	16.688179	-0.045678	3.479338
225.743711	4057.673166	16.693184	-0.045667	3.476134
225.598683	4049.596952	16.698189	-0.045636	3.472854
225.690220	4041.567307	16.703194	-0.045648	3.469597
225.516053	4033.597802	16.708199	-0.045610	3.466353
225.516119	4025.586643	16.713203	-0.045606	3.463095
225.722342	4017.612530	16.718208	-0.045639	3.459856
225.515848	4009.649786	16.723213	-0.045596	3.456605
225.419163	4001.631485	16.728218	-0.045573	3.453331
225.401878	3993.615202	16.733223	-0.045565	3.450058
225.363091	3985.641877	16.738227	-0.045553	3.446799
225.467287	3977.633259	16.743232	-0.045567	3.443526
225.156899	3969.675763	16.748237	-0.045505	3.440258
225.067904	3961.675985	16.753242	-0.045483	3.436977
225.208469	3953.687996	16.758247	-0.045504	3.433705
224.962237	3945.626692	16.763251	-0.045454	3.430387
225.068987	3937.681816	16.768256	-0.045469	3.427126
224.957687	3929.684992	16.773261	-0.045443	3.423832
224.961895	3921.710661	16.778266	-0.045439	3.420549
224.825762	3913.735125	16.783271	-0.045409	3.417257
224.664204	3905.711206	16.788275	-0.045374	3.413941
224.710647	3897.713434	16.793280	-0.045378	3.410640
224.634152	3889.727563	16.798285	-0.045359	3.407336
224.619908	3881.763146	16.803290	-0.045351	3.404040
224.566176	3873.778106	16.808295	-0.045336	3.400731
224.464694	3865.790561	16.813299	-0.045313	3.397416
224.467633	3857.796843	16.818304	-0.045308	3.394099
224.265839	3849.689179	16.823309	-0.045266	3.390724
224.378553	3841.732041	16.828314	-0.045282	3.387420
224.259814	3833.749682	16.833319	-0.045255	3.384093
224.363757	3825.790839	16.838323	-0.045269	3.380781
224.279605	3817.844481	16.843328	-0.045249	3.377464
224.062845	3809.813343	16.848333	-0.045204	3.374104
224.023942	3801.805773	16.853338	-0.045192	3.370757
224.077168	3793.838596	16.858343	-0.045197	3.367426
224.025436	3785.828642	16.863347	-0.045182	3.364071
223.962262	3777.891719	16.868352	-0.045165	3.360742
223.751694	3769.918095	16.873357	-0.045121	3.357389
223.549173	3761.913207	16.878362	-0.045079	3.354020
223.810520	3753.848188	16.883367	-0.045123	3.350639
223.642957	3745.855756	16.888371	-0.045087	3.347270
223.571635	3737.903848	16.893376	-0.045068	3.343918
223.777536	3729.894403	16.898381	-0.045102	3.340548
223.559980	3721.933543	16.903386	-0.045057	3.337180
223.605145	3713.941633	16.908391	-0.045060	3.333806
223.312490	3705.932771	16.913395	-0.045001	3.330408
223.485223	3697.953311	16.918400	-0.045028	3.327036
223.349039	3689.955270	16.923405	-0.044998	3.323641
223.279384	3681.991236	16.928410	-0.044980	3.320260
223.355635	3674.002627	16.933415	-0.044989	3.316871
223.122750	3665.982711	16.938419	-0.044941	3.313453
223.076343	3657.963446	16.943424	-0.044928	3.310038
222.858611	3649.977963	16.948429	-0.044882	3.306629
222.925280	3642.002567	16.953434	-0.044890	3.303230
222.818208	3634.032584	16.958439	-0.044865	3.299824
222.743900	3626.065762	16.963443	-0.044846	3.296417
222.837788	3618.068063	16.968448	-0.044859	3.293000
222.749855	3610.049051	16.973453	-0.044838	3.289563
222.706262	3602.071599	16.978458	-0.044825	3.286142
222.795138	3594.091252	16.983463	-0.044836	3.282721
222.680155	3586.091126	16.988467	-0.044810	3.279280
222.716225	3578.138015	16.993472	-0.044812	3.275862
222.659263	3570.110300	16.998477	-0.044796	3.272404
222.757233	3562.091483	17.003482	-0.044810	3.268953
222.790596	3554.095663	17.008487	-0.044811	3.265505
222.429560	3546.139985	17.013491	-0.044739	3.262056
222.442063	3538.176012	17.018496	-0.044737	3.258614
222.463540	3530.170592	17.023501	-0.044736	3.255150
222.343107	3522.178093	17.028506	-0.044708	3.251683
222.373799	3514.174495	17.033511	-0.044709	3.248214
222.251707	3506.192109	17.038515	-0.044682	3.244744
222.370387	3498.252045	17.043520	-0.044699	3.241298
222.189853	3490.252727	17.048525	-0.044660	3.237811
222.213272	3482.223819	17.053530	-0.044660	3.234315
222.156512	3474.198166	17.058535	-0.044644	3.230814
222.218967	3466.176553	17.063539	-0.044651	3.227315
222.227990	3458.211455	17.068544	-0.044648	3.223836
221.946386	3450.263644	17.073549	-0.044591	3.220348
221.797086	3442.300045	17.078554	-0.044558	3.216854
221.576624	3434.331225	17.083559	-0.044512	3.213352
221.887460	3426.266357	17.088563	-0.044565	3.209826
221.950334	3418.319571	17.093568	-0.044572	3.206337
221.546202	3410.348998	17.098573	-0.044492	3.202815
221.466023	3402.345320	17.103578	-0.044472	3.199288
221.658110	3394.367810	17.108583	-0.044503	3.195780
221.187457	3386.375832	17.113587	-0.044411	3.192233
221.474402	3378.355264	17.118592	-0.044459	3.188702
221.431025	3370.338346	17.123597	-0.044446	3.185155
221.392919	3362.387669	17.128602	-0.044434	3.181634
221.377094	3354.418332	17.133607	-0.044426	3.178101
221.462822	3346.393950	17.138611	-0.044438	3.174544
221.354614	3338.434446	17.143616	-0.044413	3.171003
221.184445	3330.452688	17.148621	-0.044376	3.167447
221.272729	3322.431836	17.153626	-0.044388	3.163879
221.271235	3314.492400	17.158631	-0.044382	3.160341
220.896785	3306.521888	17.163635	-0.044308	3.156768
221.030600	3298.508996	17.168640	-0.044328	3.153194
220.970161	3290.479429	17.173645	-0.044312	3.149600
220.944468	3282.492595	17.178650	-0.044302	3.146023
220.784867	3274.553036	17.183655	-0.044268	3.142457
220.747406	3266.537578	17.188659	-0.044256	3.138858
220.633157	3258.604861	17.193664	-0.044230	3.135289
220.486876	3250.579646	17.198669	-0.044197	3.131673
220.473186	3242.561770	17.203674	-0.044190	3.128062
220.517239	3234.580670	17.208679	-0.044193	3.124466
220.676189	3226.631913	17.213683	-0.044218	3.120885
220.788431	3218.637458	17.218688	-0.044234	3.117278
220.705349	3210.639914	17.223693	-0.044214	3.113656
220.601293	3202.616611	17.228698	-0.044190	3.110017
220.406031	3194.678605	17.233703	-0.044148	3.106409
220.307869	3186.707902	17.238707	-0.044125	3.102785
220.535844	3178.701500	17.243712	-0.044163	3.099157
220.524091	3170.721591	17.248717	-0.044156	3.095525
220.108149	3162.756814	17.253722	-0.044074	3.091877
220.138524	3154.753899	17.258727	-0.044074	3.088228
219.921031	3146.752681	17.263731	-0.044029	3.084564
219.805125	3138.821767	17.268736	-0.044003	3.080933
219.748580	3130.809724	17.273741	-0.043987	3.077262
219.958428	3122.757731	17.278746	-0.044021	3.073582
219.881005	3114.730249	17.283751	-0.044002	3.069895
219.620301	3106.776653	17.288755	-0.043949	3.066229
219.932686	3098.770735	17.293760	-0.044002	3.062561
219.839518	3090.802908	17.298765	-0.043980	3.058887
219.562072	3082.887293	17.303770	-0.043923	3.055225
219.730887	3074.874611	17.308775	-0.043950	3.051534
219.549863	3066.880563	17.313779	-0.043911	3.047830
219.586045	3058.902907	17.318784	-0.043913	3.044141
219.663005	3050.928671	17.323789	-0.043923	3.040450
219.629418	3042.974183	17.328794	-0.043911	3.036758
219.644675	3034.979308	17.333799	-0.043909	3.033046
219.246840	3026.983476	17.338803	-0.043831	3.029309
219.279328	3019.020588	17.343808	-0.043832	3.025603
219.275057	3011.013714	17.348813	-0.043826	3.021870
218.930215	3003.049662	17.353818	-0.043757	3.018136
218.881607	2995.075304	17.358823	-0.043743	3.014407
218.824689	2987.035029	17.363827	-0.043728	3.010642
218.696749	2979.084231	17.368832	-0.043699	3.006911
218.801322	2971.087623	17.373837	-0.043714	3.003165
218.636828	2963.124008	17.378842	-0.043678	2.999417
218.662415	2955.171577	17.383847	-0.043678	2.995679
218.701009	2947.111056	17.388851	-0.043680	2.991886
218.767598	2939.128582	17.393856	-0.043688	2.988126
218.807381	2931.117328	17.398861	-0.043690	2.984346
218.674439	2923.180799	17.403866	-0.043661	2.980589
218.758926	2915.219293	17.408871	-0.043672	2.976825
218.594009	2907.219392	17.413875	-0.043636	2.973027
218.552842	2899.222476	17.418880	-0.043624	2.969231
218.421896	2891.254631	17.423885	-0.043594	2.965439
218.157322	2883.314023	17.428890	-0.043540	2.961648
217.989615	2875.370019	17.433895	-0.043504	2.957856
217.856894	2867.348121	17.438899	-0.043475	2.954024
218.134666	2859.306091	17.443904	-0.043521	2.950199
218.035198	2851.326908	17.448909	-0.043498	2.946378
217.920001	2843.372863	17.453914	-0.043472	2.942565
217.977327	2835.387029	17.458919	-0.043478	2.938740
218.013260	2827.390488	17.463923	-0.043479	2.934903
217.734545	2819.440618	17.468928	-0.043423	2.931068
217.662670	2811.437230	17.473933	-0.043404	2.927212
217.740454	2803.459784	17.478938	-0.043414	2.923372
218.087941	2795.454830	17.483943	-0.043474	2.919528
217.911331	2787.539701	17.488947	-0.043436	2.915695
217.722209	2779.471361	17.493952	-0.043396	2.911781
217.599424	2771.477505	17.498957	-0.043368	2.907902
217.451563	2763.514511	17.503962	-0.043336	2.904032
217.457380	2755.567068	17.508967	-0.043332	2.900172
217.446009	2747.560265	17.513971	-0.043325	2.896277
217.378522	2739.575585	17.518976	-0.043308	2.892384
217.179307	2731.629117	17.523981	-0.043266	2.888498
217.157715	2723.623215	17.528986	-0.043257	2.884587
217.365613	2715.694468	17.533991	-0.043291	2.880721
217.058655	2707.707596	17.538995	-0.043229	2.876793
217.156616	2699.713861	17.544000	-0.043242	2.872879
217.230862	2691.684065	17.549005	-0.043251	2.868940
217.098752	2683.719509	17.554010	-0.043222	2.865017
216.983335	2675.783698	17.559015	-0.043195	2.861103
216.954915	2667.782569	17.564019	-0.043185	2.857156
216.855593	2659.828944	17.569024	-0.043162	2.853224
216.705231	2651.832160	17.574029	-0.043129	2.849262
216.535686	2643.867025	17.579034	-0.043093	2.845309
216.654787	2635.911150	17.584039	-0.043110	2.841371
216.221483	2627.951699	17.589043	-0.043024	2.837395
216.291734	2619.955755	17.594048	-0.043033	2.833423
216.325379	2611.916880	17.599053	-0.043034	2.829423
216.275251	2603.920194	17.604058	-0.043020	2.825433
216.361577	2595.972334	17.609063	-0.043031	2.821469
216.496335	2587.952051	17.614067	-0.043051	2.817467
216.457072	2580.009789	17.619072	-0.043039	2.813488
216.208422	2572.010768	17.624077	-0.042988	2.809463
216.309592	2564.028422	17.629082	-0.043002	2.805460
216.264935	2556.107730	17.634087	-0.042989	2.801475
215.911182	2548.144830	17.639091	-0.042918	2.797444
215.948008	2540.162632	17.644096	-0.042920	2.793421
215.909827	2532.135746	17.649101	-0.042908	2.789365
215.869878	2524.165171	17.654106	-0.042896	2.785331
215.846610	2516.219004	17.659111	-0.042887	2.781305
215.825601	2508.218897	17.664115	-0.042878	2.777246
215.873958	2500.258023	17.669120	-0.042882	2.773205
215.689978	2492.270262	17.674125	-0.042843	2.769130
215.759694	2484.284865	17.679130	-0.042851	2.765066
215.666818	2476.346130	17.684135	-0.042829	2.761010
215.528951	2468.364564	17.689139	-0.042798	2.756923
215.480088	2460.358224	17.694144	-0.042784	2.752823
215.480564	2452.312371	17.699149	-0.042780	2.748699
215.480711	2444.338190	17.704154	-0.042775	2.744607
215.460146	2436.420832	17.709159	-0.042766	2.740535
215.272133	2428.455087	17.714163	-0.042726	2.736423
215.365229	2420.459002	17.719168	-0.042739	2.732306
215.355853	2412.481046	17.724173	-0.042732	2.728186
215.246659	2404.503496	17.729178	-0.042707	2.724054
215.210588	2396.562522	17.734183	-0.042695	2.719939
215.064991	2388.618994	17.739187	-0.042663	2.715809
214.995455	2380.620887	17.744192	-0.042646	2.711650
214.881582	2372.633204	17.749197	-0.042620	2.707487
214.929510	2364.637860	17.754202	-0.042624	2.703323
214.751913	2356.720153	17.759207	-0.042586	2.699180
214.716424	2348.717632	17.764211	-0.042574	2.694994
214.742913	2340.739751	17.769216	-0.042574	2.690819
214.395015	2332.810510	17.774221	-0.042505	2.686639
214.337120	2324.817156	17.779226	-0.042489	2.682438
214.452736	2316.869310	17.784231	-0.042506	2.678265
214.519926	2308.849652	17.789235	-0.042513	2.674044
214.376566	2300.865830	17.794240	-0.042482	2.669822
214.201778	2292.893818	17.799245	-0.042444	2.665598
214.359490	2284.909925	17.804250	-0.042469	2.661382
214.343438	2276.960390	17.809255	-0.042461	2.657166
214.113321	2268.987967	17.814259	-0.042413	2.652918
214.234423	2260.992178	17.819264	-0.042431	2.648673
213.983185	2253.043676	17.824269	-0.042380	2.644422
214.054018	2245.091039	17.829274	-0.042388	2.640183
213.988213	2237.127374	17.834279	-0.042371	2.635923
213.882268	2229.120088	17.839283	-0.042346	2.631630
213.819264	2221.156986	17.844288	-0.042330	2.627356
213.855214	2213.170538	17.849293	-0.042331	2.623069
213.836140	2205.216109	17.854298	-0.042323	2.618789
213.773754	2197.271089	17.859303	-0.042307	2.614503
213.529080	2189.281140	17.864307	-0.042256	2.610175
213.657264	2181.312732	17.869312	-0.042275	2.605876
213.510672	2173.369159	17.874317	-0.042243	2.601564
213.301833	2165.417848	17.879322	-0.042199	2.597237
213.295214	2157.370525	17.884327	-0.042193	2.592865
213.394206	2149.254493	17.889331	-0.042207	2.588454
213.292600	2141.324710	17.894336	-0.042183	2.584124
213.339202	2133.393949	17.899341	-0.042187	2.579797
213.393259	2125.428764	17.904346	-0.042192	2.575444
213.311378	2117.492419	17.909351	-0.042172	2.571090
213.059170	2109.544157	17.914355	-0.042120	2.566710
213.257746	2101.576494	17.919360	-0.042152	2.562343
213.058136	2093.660485	17.924365	-0.042110	2.557970
212.973344	2085.679972	17.929370	-0.042090	2.553561
213.087947	2077.684597	17.934375	-0.042106	2.549151
212.995015	2069.709075	17.939379	-0.042084	2.544729
212.918283	2061.783650	17.944384	-0.042065	2.540328
212.725884	2053.828348	17.949389	-0.042024	2.535895
212.663452	2045.851697	17.954394	-0.042008	2.531452
212.638251	2037.881244	17.959399	-0.041998	2.527007
212.509391	2029.916316	17.964403	-0.041969	2.522550
212.901464	2021.927446	17.969408	-0.042037	2.518108
212.745879	2013.963209	17.974413	-0.042004	2.513634
212.671098	2005.966737	17.979418	-0.041985	2.509139
212.618601	1998.018364	17.984423	-0.041970	2.504665
212.572088	1990.066563	17.989427	-0.041957	2.500181
212.305472	1982.155551	17.994432	-0.041902	2.495696
212.187565	1974.159972	17.999437	-0.041876	2.491166
212.184256	1966.185074	18.004442	-0.041870	2.486648
212.360345	1958.212647	18.009447	-0.041898	2.482136
212.117170	1950.273435	18.014451	-0.041848	2.477604
211.859454	1942.334359	18.019456	-0.041795	2.473063
211.906057	1934.343295	18.024461	-0.041799	2.468506
211.795346	1926.365392	18.029466	-0.041773	2.463936
211.945955	1918.419641	18.034471	-0.041797	2.459396
211.801309	1910.466246	18.039475	-0.041765	2.454821
211.966940	1902.457778	18.044480	-0.041791	2.450229
211.872283	1894.511116	18.049485	-0.041768	2.445645
211.884931	1886.565564	18.054490	-0.041766	2.441060
211.817700	1878.627370	18.059495	-0.041749	2.436466
211.579796	1870.612013	18.064499	-0.041699	2.431804
211.405236	1862.657537	18.069504	-0.041662	2.427174
211.319600	1854.700946	18.074509	-0.041641	2.422541
211.227481	1846.740407	18.079514	-0.041619	2.417896
211.329651	1838.771576	18.084519	-0.041633	2.413252
211.175336	1830.803825	18.089523	-0.041600	2.408580
211.175904	1822.866409	18.094528	-0.041595	2.403929
211.015465	1814.941628	18.099533	-0.041560	2.399263
211.022614	1806.972883	18.104538	-0.041557	2.394576
211.020514	1798.989479	18.109543	-0.041552	2.389870
210.850846	1791.029429	18.114547	-0.041515	2.385155
210.978612	1783.068019	18.119552	-0.041534	2.380454
211.022793	1775.125309	18.124557	-0.041538	2.375748
210.842544	1767.156807	18.129562	-0.041499	2.370999
211.005433	1759.190673	18.134567	-0.041525	2.366270
210.906101	1751.240139	18.139571	-0.041501	2.361519
210.844499	1743.325348	18.144576	-0.041485	2.356783
210.670310	1735.362303	18.149581	-0.041448	2.352000
210.452435	1727.387696	18.154586	-0.041402	2.347196
210.519812	1719.434442	18.159591	-0.041410	2.342419
210.445229	1711.478847	18.164595	-0.041391	2.337618
210.465877	1703.522813	18.169600	-0.041390	2.332816
210.353641	1695.568755	18.174605	-0.041365	2.327994
210.218048	1687.611280	18.179610	-0.041334	2.323157
210.083706	1679.700822	18.184615	-0.041305	2.318340
210.158871	1671.707818	18.189619	-0.041314	2.313479
210.126422	1663.750114	18.194624	-0.041303	2.308621
209.893039	1655.812745	18.199629	-0.041255	2.303748
209.744681	1647.887004	18.204634	-0.041222	2.298879
209.791548	1639.932766	18.209639	-0.041226	2.293998
209.542683	1631.972524	18.214643	-0.041175	2.289079
209.624837	1624.004142	18.219648	-0.041185	2.284171
209.634459	1616.062323	18.224653	-0.041182	2.279264
209.460336	1608.140080	18.229658	-0.041145	2.274342
209.470431	1600.093031	18.234663	-0.041142	2.269348
209.467793	1592.120832	18.239667	-0.041137	2.264388
209.214375	1584.234163	18.244672	-0.041085	2.259450
209.092884	1576.296897	18.249677	-0.041057	2.254480
208.998902	1568.322330	18.254682	-0.041035	2.249478
208.997639	1560.391381	18.259687	-0.041030	2.244500
208.775371	1552.474652	18.264691	-0.040984	2.239501
208.942863	1544.510623	18.269696	-0.041010	2.234495
209.099478	1536.510553	18.274701	-0.041034	2.229455
208.884298	1528.574407	18.279706	-0.040989	2.224410
208.911053	1520.655361	18.284711	-0.040990	2.219386
208.770964	1512.717365	18.289715	-0.040959	2.214324
208.726762	1504.764300	18.294720	-0.040946	2.209249
208.555641	1496.830089	18.299725	-0.040909	2.204163
208.615846	1488.890168	18.304730	-0.040915	2.199083
208.635223	1480.953178	18.309735	-0.040914	2.193989
208.355092	1472.981031	18.314739	-0.040857	2.188833
208.288086	1465.046234	18.319744	-0.040840	2.183708
208.363121	1457.098122	18.324749	-0.040849	2.178576
208.398621	1449.143011	18.329754	-0.040851	2.173424
208.248767	1441.218211	18.334759	-0.040818	2.168262
208.194423	1433.280809	18.339763	-0.040803	2.163088
208.247338	1425.342579	18.344768	-0.040808	2.157911
208.082609	1417.416069	18.349773	-0.040772	2.152709
208.106854	1409.435676	18.354778	-0.040772	2.147477
208.317991	1401.479460	18.359783	-0.040807	2.142266
208.063198	1393.588678	18.364787	-0.040754	2.137041
207.992144	1385.657704	18.369792	-0.040736	2.131794
207.975508	1377.710452	18.374797	-0.040728	2.126528
207.738618	1369.794402	18.379802	-0.040679	2.121249
207.870883	1361.857629	18.384807	-0.040699	2.115979
207.754566	1353.857026	18.389811	-0.040673	2.110628
207.554293	1345.928295	18.394816	-0.040631	2.105304
207.423648	1338.024310	18.399821	-0.040601	2.099990
207.461171	1330.082645	18.404826	-0.040604	2.094654
207.498931	1322.132923	18.409831	-0.040606	2.089298
207.330162	1314.207949	18.414835	-0.040570	2.083925
207.015486	1306.315321	18.419840	-0.040506	2.078546
207.043418	1298.374368	18.424845	-0.040507	2.073153
207.059824	1290.410400	18.429850	-0.040505	2.067730
207.153274	1282.477944	18.434855	-0.040517	2.062322
207.053835	1274.550484	18.439859	-0.040494	2.056884
207.086769	1266.617383	18.444864	-0.040495	2.051440
206.979631	1258.696171	18.449869	-0.040471	2.045976
206.670964	1250.793482	18.454874	-0.040408	2.040490
207.072417	1242.841608	18.459879	-0.040478	2.035028
206.857377	1234.888099	18.464883	-0.040433	2.029486
206.780117	1226.971085	18.469888	-0.040414	2.023969
206.804380	1219.052884	18.474893	-0.040414	2.018446
206.682044	1211.132533	18.479898	-0.040386	2.012892
206.486932	1203.218894	18.484903	-0.040345	2.007319
206.378462	1195.296792	18.489907	-0.040320	2.001734
206.397284	1187.383713	18.494912	-0.040319	1.996152
206.398663	1179.446625	18.499917	-0.040314	1.990537
206.195740	1171.511559	18.504922	-0.040272	1.984885
206.341660	1163.603114	18.509927	-0.040294	1.979273
206.078321	1155.706359	18.514931	-0.040240	1.973610
205.957775	1147.768653	18.519936	-0.040213	1.967916
205.967844	1139.856386	18.524941	-0.040210	1.962238
205.913064	1131.946377	18.529946	-0.040195	1.956539
205.607548	1124.026427	18.534951	-0.040133	1.950788
205.759421	1116.041578	18.539955	-0.040157	1.945023
205.873725	1108.123880	18.544960	-0.040173	1.939285
205.917803	1100.210527	18.549965	-0.040176	1.933526
205.682133	1092.297770	18.554970	-0.040128	1.927720
205.770817	1084.394744	18.559975	-0.040139	1.921939
205.693302	1076.490877	18.564979	-0.040120	1.916121
205.477356	1068.593933	18.569984	-0.040075	1.910275
205.526546	1060.679673	18.574989	-0.040080	1.904428
205.367813	1052.776631	18.579994	-0.040045	1.898548
205.335685	1044.869312	18.584999	-0.040034	1.892661
205.092285	1036.964419	18.590003	-0.039984	1.886733
205.022579	1029.074750	18.595008	-0.039967	1.880818
205.093273	1021.161757	18.600013	-0.039975	1.874883
204.799103	1013.248951	18.605018	-0.039915	1.868887
204.856048	1005.334492	18.610023	-0.039921	1.862910
204.748136	997.432341	18.615027	-0.039896	1.856905
204.746978	989.509138	18.620032	-0.039891	1.850877
204.648609	981.620290	18.625037	-0.039868	1.844844
204.674744	973.713551	18.630042	-0.039868	1.838792
204.550915	965.837988	18.635047	-0.039840	1.832726
204.353303	957.942517	18.640051	-0.039799	1.826616
204.348480	950.037232	18.645056	-0.039793	1.820501
204.460723	942.121126	18.650061	-0.039809	1.814371
204.113579	934.268199	18.655066	-0.039740	1.808214
204.161448	926.364621	18.660071	-0.039744	1.802044
204.131834	918.472600	18.665075	-0.039733	1.795852
204.053847	910.523584	18.670080	-0.039714	1.789588
203.835087	902.652505	18.675085	-0.039669	1.783347
203.708715	894.766256	18.680090	-0.039640	1.777083
203.781849	886.863696	18.685095	-0.039649	1.770808
203.535330	879.000188	18.690099	-0.039598	1.764502
203.535412	871.115786	18.695104	-0.039594	1.758188
203.679518	863.201483	18.700109	-0.039616	1.751846
203.446382	855.328311	18.705114	-0.039567	1.745465
203.434535	847.464832	18.710119	-0.039560	1.739097
203.633136	839.535179	18.715123	-0.039593	1.732679
203.509971	831.672001	18.720128	-0.039565	1.726250
203.286971	823.836935	18.725133	-0.039519	1.719807
203.148325	815.973369	18.730138	-0.039488	1.713328
203.053931	808.082605	18.735143	-0.039466	1.706807
202.881686	800.215124	18.740147	-0.039429	1.700270
202.922651	792.337960	18.745152	-0.039432	1.693727
203.028318	784.429184	18.750157	-0.039446	1.687142
202.723829	776.597841	18.755162	-0.039385	1.680541
202.586918	768.762423	18.760167	-0.039355	1.673933
202.510361	760.865234	18.765171	-0.039336	1.667254
202.605797	752.979353	18.770176	-0.039349	1.660582
202.554544	745.128030	18.775181	-0.039334	1.653892
202.590595	737.232765	18.780186	-0.039336	1.647149
202.623109	729.382269	18.785191	-0.039338	1.640417
202.388770	721.553181	18.790195	-0.039289	1.633638
202.282246	713.643801	18.795200	-0.039265	1.626780
202.489392	705.757771	18.800205	-0.039298	1.619956
202.202342	697.947632	18.805210	-0.039240	1.613100
202.169659	690.090307	18.810215	-0.039229	1.606210
202.057174	682.252223	18.815219	-0.039204	1.599296
202.003801	674.419195	18.820224	-0.039189	1.592364
201.922164	666.559019	18.825229	-0.039169	1.585374
201.709863	658.747247	18.830234	-0.039125	1.578377
201.754156	650.892170	18.835239	-0.039128	1.571347
201.479423	643.073289	18.840243	-0.039072	1.564272
201.338790	635.264694	18.845248	-0.039041	1.557194
201.360945	627.402197	18.850253	-0.039041	1.550058
201.251373	619.555325	18.855258	-0.039015	1.542884
201.182851	611.731866	18.860263	-0.038998	1.535704
201.186573	603.877601	18.865267	-0.038994	1.528473
201.300578	596.030348	18.870272	-0.039010	1.521230
201.166713	588.241858	18.875277	-0.038981	1.513970
200.943020	580.425083	18.880282	-0.038934	1.506635
201.121448	572.585036	18.885287	-0.038963	1.499303
200.959231	564.779282	18.890291	-0.038928	1.491916
200.755828	556.981573	18.895296	-0.038885	1.484493
200.898031	549.158053	18.900301	-0.038907	1.477061
200.592156	541.340944	18.905306	-0.038845	1.469528
200.522544	533.532829	18.910311	-0.038827	1.462003
200.485375	525.726090	18.915315	-0.038816	1.454444
200.375261	517.929130	18.920320	-0.038791	1.446844
200.079270	510.184681	18.925325	-0.038731	1.439225
200.035795	502.379333	18.930330	-0.038718	1.431547
200.145585	494.565124	18.935335	-0.038734	1.423843
199.990715	486.789544	18.940339	-0.038700	1.416093
199.843864	479.013523	18.945344	-0.038668	1.408300
199.916295	471.210640	18.950349	-0.038677	1.400474
199.795558	463.447146	18.955354	-0.038649	1.392611
199.501473	455.693350	18.960359	-0.038590	1.384685
199.445504	447.921007	18.965363	-0.038575	1.376733
199.605869	440.110846	18.970368	-0.038600	1.368734
199.343622	432.384804	18.975373	-0.038546	1.360702
199.148713	424.648912	18.980378	-0.038505	1.352624
199.200630	416.865022	18.985383	-0.038510	1.344490
199.233227	409.106853	18.990387	-0.038512	1.336330
199.140268	401.360171	18.995392	-0.038490	1.328110
199.038073	393.632233	19.000397	-0.038466	1.319857
198.951375	385.829577	19.005402	-0.038445	1.311475
199.020831	378.023145	19.010407	-0.038453	1.303062
198.814315	370.321425	19.015411	-0.038410	1.294659
198.880010	362.575489	19.020416	-0.038418	1.286203
198.867078	354.883650	19.025421	-0.038411	1.277735
198.588506	347.203624	19.030426	-0.038354	1.269175
198.464254	339.508931	19.035431	-0.038326	1.260569
198.297551	331.828326	19.040435	-0.038291	1.251911
198.165925	324.140991	19.045440	-0.038261	1.243192
198.190838	316.441047	19.050445	-0.038261	1.234428
198.009217	308.744954	19.055450	-0.038223	1.225565
198.190695	301.040255	19.060455	-0.038252	1.216699
197.862238	293.394930	19.065459	-0.038186	1.207736
197.979605	285.706192	19.070464	-0.038203	1.198744
197.803469	278.070903	19.075469	-0.038166	1.189688
197.476711	270.449297	19.080474	-0.038101	1.180548
197.595248	262.774251	19.085479	-0.038118	1.171364
197.327445	255.161347	19.090483	-0.038063	1.162102
197.212279	247.527998	19.095488	-0.038037	1.152774
197.137378	239.868713	19.100493	-0.038019	1.143345
197.232882	232.217719	19.105498	-0.038032	1.133885
197.131208	224.614286	19.110503	-0.038008	1.124362
196.931583	217.043223	19.115507	-0.037967	1.114777
196.932031	209.428528	19.120512	-0.037962	1.105098
196.839647	201.857877	19.125517	-0.037940	1.095369
196.599979	194.297835	19.130522	-0.037891	1.085534
196.416224	186.765855	19.135527	-0.037852	1.075658
196.399282	179.175453	19.140531	-0.037845	1.065651
196.058902	171.676881	19.145536	-0.037777	1.055597
195.791897	164.165024	19.150541	-0.037722	1.045446
195.772189	156.624115	19.155546	-0.037714	1.035214
195.805412	149.087519	19.160551	-0.037716	1.024898
195.518899	141.621597	19.165555	-0.037658	1.014499
195.310394	134.143840	19.170560	-0.037615	1.003994
195.362884	126.641470	19.175565	-0.037620	0.993407
195.051816	119.177546	19.180570	-0.037557	0.982671
195.125674	111.700558	19.185575	-0.037567	0.971894
195.113962	104.247544	19.190579	-0.037560	0.961010
195.071242	96.825532	19.195584	-0.037547	0.950039
194.912945	89.437645	19.200589	-0.037513	0.938961
194.727344	82.055312	19.205594	-0.037474	0.927751
194.603885	74.706799	19.210599	-0.037447	0.916473
194.397600	67.350466	19.215603	-0.037404	0.905020
194.188113	60.269255	19.220608	-0.037361	0.893853