Thu Mar 11 18:04:31 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.679938	-0.036546	0.000000	-0.000054	0.725212

0.626718	-0.024245	0.005005	-0.000045	0.725218
0.422175	0.008169	0.010010	-0.000007	0.725210
0.560620	-0.082856	0.015014	-0.000033	0.725081
0.330839	-0.140634	0.020019	0.000010	0.724888
0.250005	-0.126051	0.025024	0.000024	0.724889
0.384487	-0.146928	0.030029	-0.000001	0.724896
0.362944	-0.148486	0.035034	0.000003	0.724886
0.340172	-0.140449	0.040038	0.000007	0.724894
0.437910	-0.161049	0.045043	-0.000012	0.724888
0.504665	-0.172820	0.050048	-0.000024	0.724889
0.595288	-0.186128	0.055053	-0.000041	0.724895
0.281929	-0.135536	0.060058	0.000017	0.724885
0.483299	-0.166805	0.065062	-0.000021	0.724895
0.378786	-0.148844	0.070067	-0.000002	0.724894
0.241391	-0.129099	0.075072	0.000023	0.724885
0.314852	-0.268993	0.080077	0.000010	0.724637
0.061919	-0.249256	0.085082	0.000056	0.724588
0.140509	-0.259346	0.090086	0.000041	0.724597
0.268693	-0.285245	0.095091	0.000017	0.724591
0.409810	-0.311692	0.100096	-0.000009	0.724589
0.485595	-0.323077	0.105101	-0.000024	0.724593
0.422324	-0.361907	0.110106	-0.000012	0.724496
0.278495	-0.455913	0.115110	0.000015	0.724262
0.442988	-0.487917	0.120115	-0.000016	0.724257
0.024373	-0.413755	0.125120	0.000061	0.724257
0.105082	-0.422830	0.130125	0.000046	0.724268
0.157590	-0.460647	0.135130	0.000036	0.724213
0.328461	-0.621432	0.140134	0.000004	0.723958
0.303456	-0.620135	0.145139	0.000009	0.723952
0.572489	-0.669794	0.150144	-0.000042	0.723949
0.575598	-0.675097	0.155149	-0.000043	0.723940
0.505006	-0.821003	0.160154	-0.000030	0.723630
0.547344	-0.824367	0.165158	-0.000038	0.723639
0.384963	-0.797536	0.170163	-0.000008	0.723635
-0.076167	-0.785373	0.175168	0.000078	0.723499
-0.021150	-0.873771	0.180173	0.000067	0.723345
-0.105566	-0.863328	0.185178	0.000083	0.723337
-0.155381	-0.851759	0.190182	0.000092	0.723343
-0.073982	-1.001751	0.195187	0.000076	0.723077
0.268263	-1.099347	0.200192	0.000013	0.723006
0.307802	-1.103967	0.205197	0.000005	0.723011
0.029090	-1.160065	0.210202	0.000057	0.722804
0.125775	-1.231506	0.215206	0.000038	0.722698
0.177247	-1.243423	0.220211	0.000029	0.722693
-0.069296	-1.315619	0.225216	0.000074	0.722466
0.026543	-1.380087	0.230221	0.000056	0.722373
-0.069343	-1.366282	0.235226	0.000074	0.722368
-0.000414	-1.502585	0.240230	0.000061	0.722125
-0.072704	-1.515356	0.245235	0.000074	0.722075
-0.131633	-1.536504	0.250240	0.000085	0.722013
-0.473396	-1.609786	0.255245	0.000148	0.721750
-1.006698	-1.520552	0.260250	0.000247	0.721739
-0.743531	-1.618421	0.265254	0.000198	0.721639
-0.738827	-1.720292	0.270259	0.000197	0.721441
-0.834168	-1.705706	0.275264	0.000214	0.721437
-1.259228	-1.731695	0.280269	0.000293	0.721238
-2.285201	-1.609177	0.285274	0.000484	0.721120
-2.141044	-1.633149	0.290278	0.000457	0.721124
-2.042228	-1.712542	0.295283	0.000438	0.721003
-2.819351	-1.638440	0.300288	0.000583	0.720877
-2.631420	-1.667670	0.305293	0.000547	0.720885
-3.004087	-1.632696	0.310298	0.000617	0.720824
-3.497405	-1.686170	0.315302	0.000708	0.720547
-3.545249	-1.680197	0.320307	0.000717	0.720542
-3.713095	-1.652258	0.325312	0.000748	0.720539
-3.870759	-1.695916	0.330317	0.000777	0.720398
-4.776632	-1.625023	0.335322	0.000945	0.720220
-4.198259	-1.723948	0.340326	0.000837	0.720229
-4.624783	-1.649863	0.345331	0.000917	0.720226
-4.962404	-1.636077	0.350336	0.000979	0.720135
-5.495946	-1.656096	0.355341	0.001078	0.719909
-5.180302	-1.717904	0.360346	0.001019	0.719898
-5.577442	-1.645285	0.365350	0.001093	0.719903
-5.870141	-1.595505	0.370355	0.001147	0.719898
-5.818792	-1.688675	0.375360	0.001137	0.719733
-6.546868	-1.622979	0.380365	0.001273	0.719608
-6.490419	-1.636764	0.385370	0.001262	0.719601
-6.470499	-1.636757	0.390374	0.001258	0.719608
-6.524334	-1.628208	0.395379	0.001268	0.719607
-6.488944	-1.701199	0.400384	0.001261	0.719476
-7.321317	-1.654070	0.405389	0.001416	0.719277
-7.190926	-1.681972	0.410394	0.001391	0.719268
-7.702087	-1.587858	0.415398	0.001486	0.719275
-7.659374	-1.595673	0.420403	0.001478	0.719275
-7.483711	-1.629460	0.425408	0.001445	0.719270
-7.581085	-1.705326	0.430413	0.001463	0.719087
-8.954345	-1.526081	0.435418	0.001718	0.718959
-8.345412	-1.632485	0.440422	0.001604	0.718963
-8.109046	-1.675343	0.445427	0.001560	0.718962
-8.717102	-1.570855	0.450432	0.001673	0.718955
-8.380684	-1.625124	0.455437	0.001610	0.718967
-8.294666	-1.689507	0.460442	0.001594	0.718870
-9.114165	-1.656597	0.465446	0.001746	0.718648
-8.874823	-1.700737	0.470451	0.001701	0.718645
-9.438407	-1.603968	0.475456	0.001806	0.718639
-9.090375	-1.660507	0.480461	0.001741	0.718650
-9.262493	-1.635160	0.485466	0.001773	0.718640
-9.405622	-1.615372	0.490470	0.001799	0.718629
-9.750457	-1.690717	0.495475	0.001863	0.718360
-10.205031	-1.612214	0.500480	0.001948	0.718355
-10.375192	-1.577885	0.505485	0.001979	0.718364
-9.965433	-1.655105	0.510490	0.001902	0.718356
-10.302444	-1.593035	0.515494	0.001965	0.718360
-10.394243	-1.577327	0.520499	0.001982	0.718360
-10.140712	-1.678656	0.525504	0.001934	0.718249
-10.646120	-1.701462	0.530509	0.002028	0.718027
-11.099011	-1.626693	0.535514	0.002112	0.718016
-11.460409	-1.560872	0.540518	0.002179	0.718019
-11.160723	-1.614497	0.545523	0.002123	0.718019
-11.297386	-1.594116	0.550528	0.002148	0.718012
-11.178264	-1.609772	0.555533	0.002126	0.718023
-11.090255	-1.679066	0.560538	0.002109	0.717918
-12.328821	-1.565897	0.565542	0.002340	0.717706
-12.126437	-1.602191	0.570547	0.002302	0.717706
-12.511654	-1.537024	0.575552	0.002373	0.717700
-12.063514	-1.611405	0.580557	0.002289	0.717711
-12.255840	-1.582529	0.585562	0.002325	0.717701
-12.372648	-1.559404	0.590566	0.002346	0.717706
-11.934716	-1.636745	0.595571	0.002265	0.717708
-12.515360	-1.661018	0.600576	0.002373	0.717456
-13.483595	-1.522632	0.605581	0.002553	0.717389
-13.108204	-1.594401	0.610586	0.002482	0.717379
-12.616162	-1.680238	0.615590	0.002391	0.717384
-13.098305	-1.594842	0.620595	0.002480	0.717383
-13.234444	-1.574708	0.625600	0.002505	0.717375
-12.712168	-1.663444	0.630605	0.002408	0.717384
-13.118921	-1.670015	0.635610	0.002483	0.717229
-14.137499	-1.560642	0.640614	0.002672	0.717087
-13.446986	-1.684478	0.645619	0.002544	0.717085
-14.044414	-1.581425	0.650624	0.002655	0.717079
-14.043498	-1.576864	0.655629	0.002654	0.717089
-13.803977	-1.623760	0.660634	0.002609	0.717081
-13.845146	-1.614110	0.665638	0.002617	0.717086
-14.062232	-1.665710	0.670643	0.002657	0.716908
-15.063849	-1.565197	0.675648	0.002843	0.716754
-14.413068	-1.676318	0.680653	0.002722	0.716764
-14.887973	-1.596743	0.685658	0.002810	0.716755
-15.030032	-1.570975	0.690662	0.002836	0.716756
-14.605802	-1.645291	0.695667	0.002757	0.716759
-15.144592	-1.553271	0.700672	0.002857	0.716752
-15.151606	-1.576283	0.705677	0.002858	0.716704
-15.804644	-1.591959	0.710682	0.002979	0.716444
-15.652388	-1.617554	0.715686	0.002951	0.716447
-16.096972	-1.536950	0.720691	0.003033	0.716450
-16.210978	-1.519136	0.725696	0.003054	0.716446
-15.672912	-1.613456	0.730701	0.002954	0.716449
-15.934744	-1.569861	0.735706	0.003002	0.716444
-15.936786	-1.565921	0.740710	0.003002	0.716452
-15.634345	-1.679714	0.745715	0.002946	0.716333
-16.996268	-1.540437	0.750720	0.003199	0.716129
-16.552559	-1.615942	0.755725	0.003116	0.716137
-17.130697	-1.517142	0.760730	0.003224	0.716129
-16.961068	-1.545833	0.765734	0.003192	0.716132
-16.744855	-1.582822	0.770739	0.003151	0.716136
-17.062511	-1.531250	0.775744	0.003210	0.716126
-16.596296	-1.608913	0.780749	0.003123	0.716138
-17.045053	-1.643142	0.785754	0.003206	0.715912
-17.995593	-1.488239	0.790758	0.003383	0.715884
-17.535267	-1.571434	0.795763	0.003297	0.715882
-17.189707	-1.635404	0.800768	0.003233	0.715878
-17.480501	-1.577824	0.805773	0.003286	0.715890
-17.717771	-1.540372	0.810778	0.003330	0.715881
-17.229533	-1.638621	0.815782	0.003239	0.715859
-18.343875	-1.596081	0.820787	0.003446	0.715550
-18.713867	-1.534747	0.825792	0.003515	0.715541
-18.606552	-1.548994	0.830797	0.003495	0.715552
-18.381729	-1.592716	0.835802	0.003453	0.715545
-18.666706	-1.540228	0.840806	0.003505	0.715549
-18.455173	-1.577174	0.845811	0.003466	0.715551
-18.250076	-1.618720	0.850816	0.003427	0.715541
-18.736725	-1.662427	0.855821	0.003518	0.715283
-19.727102	-1.510756	0.860826	0.003702	0.715234
-19.442461	-1.562104	0.865830	0.003649	0.715234
-19.240648	-1.598185	0.870835	0.003611	0.715234
-19.528637	-1.550590	0.875840	0.003664	0.715227
-19.272271	-1.591472	0.880845	0.003616	0.715237
-19.158713	-1.615726	0.885850	0.003595	0.715229
-20.054089	-1.583410	0.890854	0.003761	0.714978
-20.557307	-1.528382	0.895859	0.003855	0.714909
-20.236703	-1.589088	0.900864	0.003795	0.714903
-20.363696	-1.562149	0.905869	0.003818	0.714912
-20.706726	-1.504706	0.910874	0.003882	0.714905
-20.500909	-1.539339	0.915878	0.003843	0.714910
-20.230805	-1.586132	0.920883	0.003793	0.714913
-20.658838	-1.519641	0.925888	0.003872	0.714894
-21.052914	-1.589815	0.930893	0.003945	0.714616
-21.056204	-1.595057	0.935898	0.003946	0.714605
-21.684876	-1.480158	0.940902	0.004062	0.714611
-21.172843	-1.570133	0.945907	0.003967	0.714614
-21.138793	-1.581203	0.950912	0.003960	0.714604
-21.325380	-1.544120	0.955917	0.003995	0.714612
-21.397309	-1.533793	0.960922	0.004008	0.714608
-21.308335	-1.681242	0.965926	0.003991	0.714347
-22.159476	-1.563761	0.970931	0.004149	0.714280
-22.500684	-1.508326	0.975936	0.004212	0.714270
-21.919075	-1.606810	0.980941	0.004104	0.714280
-22.098247	-1.579497	0.985946	0.004137	0.714272
-22.455795	-1.511328	0.990950	0.004203	0.714281
-22.394215	-1.523096	0.995955	0.004192	0.714280
-22.388043	-1.603645	1.000960	0.004190	0.714123
-23.206840	-1.532446	1.005965	0.004342	0.713975
-23.271405	-1.525234	1.010970	0.004354	0.713967
-23.435602	-1.493950	1.015974	0.004384	0.713971
-23.291798	-1.519150	1.020979	0.004357	0.713972
-23.304607	-1.521749	1.025984	0.004360	0.713963
-23.272859	-1.523371	1.030989	0.004353	0.713972
-23.150289	-1.549304	1.035994	0.004330	0.713964
-23.514501	-1.618047	1.040998	0.004398	0.713699
-24.107682	-1.534514	1.046003	0.004508	0.713655
-24.286084	-1.506352	1.051008	0.004541	0.713649
-23.802016	-1.592019	1.056013	0.004451	0.713650
-24.578841	-1.455118	1.061018	0.004595	0.713648
-24.316727	-1.502143	1.066022	0.004546	0.713648
-23.911274	-1.571999	1.071027	0.004470	0.713653
-24.366141	-1.537011	1.076032	0.004555	0.713562
-24.995285	-1.524883	1.081037	0.004671	0.713364
-24.692552	-1.582481	1.086042	0.004615	0.713357
-25.307078	-1.474729	1.091046	0.004729	0.713354
-25.106917	-1.508520	1.096051	0.004691	0.713358
-24.763780	-1.572650	1.101056	0.004627	0.713353
-24.563460	-1.605960	1.106061	0.004590	0.713358
-25.350905	-1.499022	1.111066	0.004736	0.713292
-26.150097	-1.494048	1.116070	0.004885	0.713019
-25.370960	-1.630333	1.121075	0.004739	0.713024
-26.069810	-1.509043	1.126080	0.004869	0.713019
-25.808806	-1.551442	1.131085	0.004820	0.713027
-25.673820	-1.579348	1.136090	0.004795	0.713020
-26.126599	-1.498372	1.141094	0.004879	0.713021
-26.047353	-1.511366	1.146099	0.004864	0.713024
-26.411345	-1.587799	1.151104	0.004932	0.712743
-26.728399	-1.546333	1.156109	0.004990	0.712714
-26.993773	-1.502157	1.161114	0.005039	0.712708
-26.815382	-1.534347	1.166118	0.005006	0.712708
-26.747878	-1.544113	1.171123	0.004993	0.712713
-27.071975	-1.491591	1.176128	0.005053	0.712703
-26.996602	-1.500485	1.181133	0.005039	0.712712
-26.812738	-1.604949	1.186138	0.005005	0.712570
-27.750507	-1.531290	1.191142	0.005179	0.712384
-27.538570	-1.567694	1.196147	0.005139	0.712388
-28.016374	-1.487859	1.201152	0.005228	0.712378
-27.822973	-1.518335	1.206157	0.005192	0.712386
-27.733479	-1.536488	1.211162	0.005175	0.712382
-28.110788	-1.471111	1.216166	0.005245	0.712379
-27.438675	-1.615801	1.221171	0.005119	0.712330
-28.637321	-1.525349	1.226176	0.005342	0.712085
-28.702727	-1.511005	1.231181	0.005354	0.712091
-28.885333	-1.482943	1.236186	0.005388	0.712082
-28.666287	-1.521007	1.241190	0.005347	0.712085
-28.592115	-1.532121	1.246195	0.005333	0.712089
-28.816482	-1.497167	1.251200	0.005374	0.712080
-28.379373	-1.570287	1.256205	0.005293	0.712090
-29.050530	-1.599072	1.261210	0.005417	0.711795
-29.968623	-1.454005	1.266214	0.005588	0.711758
-29.366083	-1.559153	1.271219	0.005476	0.711763
-29.328455	-1.569158	1.276224	0.005468	0.711757
-29.344055	-1.564042	1.281229	0.005471	0.711762
-29.606918	-1.518819	1.286234	0.005520	0.711759
-29.542916	-1.530980	1.291238	0.005507	0.711758
-29.897914	-1.590826	1.296243	0.005573	0.711513
-30.869167	-1.449305	1.301248	0.005754	0.711451
-30.311185	-1.545890	1.306253	0.005650	0.711457
-30.191575	-1.569016	1.311258	0.005627	0.711454
-30.830210	-1.456479	1.316262	0.005746	0.711452
-30.202056	-1.566195	1.321267	0.005629	0.711457
-30.407755	-1.533622	1.326272	0.005667	0.711449
-30.789570	-1.558161	1.331277	0.005737	0.711265
-31.740082	-1.454426	1.336282	0.005914	0.711135
-31.259736	-1.540505	1.341286	0.005825	0.711134
-31.386879	-1.513989	1.346291	0.005848	0.711142
-31.720948	-1.459555	1.351296	0.005910	0.711133
-31.012045	-1.582138	1.356301	0.005778	0.711141
-31.081922	-1.571263	1.361306	0.005790	0.711138
-31.727682	-1.492728	1.366310	0.005910	0.711065
-32.202695	-1.504944	1.371315	0.005999	0.710873
-32.125065	-1.524146	1.376320	0.005984	0.710862
-32.151717	-1.515304	1.381325	0.005989	0.710871
-32.035038	-1.540449	1.386330	0.005967	0.710863
-31.839923	-1.575231	1.391334	0.005930	0.710863
-32.081655	-1.528648	1.396339	0.005975	0.710871
-32.518581	-1.524133	1.401344	0.006056	0.710725
-33.178904	-1.502728	1.406349	0.006178	0.710533
-32.740129	-1.583902	1.411354	0.006097	0.710528
-33.389755	-1.469281	1.416358	0.006217	0.710526
-33.113926	-1.514423	1.421363	0.006166	0.710534
-33.032541	-1.534292	1.426368	0.006150	0.710524
-33.090288	-1.519716	1.431373	0.006161	0.710533
-33.229689	-1.527747	1.436378	0.006186	0.710468
-33.937568	-1.528724	1.441382	0.006318	0.710214
-33.754307	-1.560068	1.446387	0.006284	0.710218
-34.470712	-1.435339	1.451392	0.006417	0.710212
-33.982557	-1.520120	1.456397	0.006326	0.710217
-33.910015	-1.535989	1.461402	0.006312	0.710212
-34.429266	-1.441591	1.466406	0.006408	0.710216
-34.064958	-1.504809	1.471411	0.006340	0.710220
-34.267594	-1.605578	1.476416	0.006378	0.709947
-34.923445	-1.513499	1.481421	0.006499	0.709898
-35.139143	-1.477102	1.486426	0.006539	0.709894
-34.941524	-1.514441	1.491430	0.006502	0.709890
-34.967141	-1.506727	1.496435	0.006507	0.709897
-35.245284	-1.461504	1.501440	0.006558	0.709889
-34.782257	-1.539584	1.506445	0.006472	0.709898
-34.949695	-1.597505	1.511450	0.006503	0.709723
-36.081440	-1.461032	1.516454	0.006713	0.709593
-35.498356	-1.561839	1.521459	0.006604	0.709600
-35.771416	-1.517636	1.526464	0.006655	0.709592
-35.830590	-1.503396	1.531469	0.006666	0.709600
-35.565786	-1.553333	1.536474	0.006616	0.709595
-35.818093	-1.509512	1.541478	0.006663	0.709593
-35.664409	-1.662579	1.546483	0.006634	0.709342
-36.790970	-1.503783	1.551488	0.006844	0.709258
-36.767512	-1.504116	1.556493	0.006839	0.709266
-36.445682	-1.562500	1.561498	0.006779	0.709265
-37.040228	-1.457527	1.566502	0.006889	0.709263
-36.849578	-1.488944	1.571507	0.006853	0.709269
-36.714909	-1.517443	1.576512	0.006828	0.709261
-36.859337	-1.590532	1.581517	0.006855	0.709063
-37.905082	-1.458204	1.586522	0.007049	0.708956
-37.592297	-1.514548	1.591526	0.006991	0.708955
-37.191166	-1.583480	1.596531	0.006916	0.708960
-37.792512	-1.481113	1.601536	0.007027	0.708951
-37.590334	-1.513651	1.606541	0.006990	0.708959
-37.367283	-1.553846	1.611546	0.006948	0.708958
-37.912126	-1.555137	1.616550	0.007049	0.708762
-38.643401	-1.482997	1.621555	0.007185	0.708646
-38.417163	-1.527931	1.626560	0.007143	0.708637
-38.510667	-1.508590	1.631565	0.007160	0.708643
-38.576356	-1.498532	1.636570	0.007172	0.708640
-38.562589	-1.502558	1.641574	0.007169	0.708637
-38.135455	-1.576751	1.646579	0.007089	0.708642
-38.648795	-1.551585	1.651584	0.007184	0.708509
-39.513114	-1.477911	1.656589	0.007345	0.708349
-38.903984	-1.586453	1.661594	0.007231	0.708349
-39.451403	-1.490806	1.666598	0.007333	0.708346
-39.143994	-1.541793	1.671603	0.007276	0.708354
-39.110414	-1.551609	1.676608	0.007269	0.708347
-39.028081	-1.564310	1.681613	0.007253	0.708351
-39.453895	-1.607672	1.686618	0.007333	0.708113
-40.615184	-1.453182	1.691622	0.007548	0.708008
-39.978577	-1.563042	1.696627	0.007430	0.708016
-40.157014	-1.536079	1.701632	0.007463	0.708007
-40.519919	-1.466231	1.706637	0.007530	0.708018
-40.239571	-1.518744	1.711642	0.007477	0.708013
-40.219707	-1.524478	1.716646	0.007473	0.708009
-40.318728	-1.569163	1.721651	0.007492	0.707885
-41.298903	-1.488922	1.726656	0.007674	0.707696
-40.945144	-1.549889	1.731661	0.007608	0.707700
-41.337354	-1.480344	1.736666	0.007681	0.707700
-41.464943	-1.460107	1.741670	0.007704	0.707696
-41.059731	-1.528494	1.746675	0.007628	0.707704
-41.336799	-1.483480	1.751680	0.007680	0.707695
-41.308699	-1.486362	1.756685	0.007674	0.707700
-41.450679	-1.616992	1.761690	0.007700	0.707388
-42.223144	-1.488808	1.766694	0.007844	0.707369
-42.342856	-1.461494	1.771699	0.007866	0.707382
-41.891067	-1.545537	1.776704	0.007782	0.707375
-42.056171	-1.515266	1.781709	0.007812	0.707377
-42.161428	-1.496091	1.786714	0.007831	0.707379
-42.271836	-1.479030	1.791718	0.007852	0.707374
-41.854534	-1.652085	1.796723	0.007774	0.707176
-43.082051	-1.482750	1.801728	0.008002	0.707078
-43.034338	-1.488353	1.806733	0.007993	0.707084
-42.781638	-1.533760	1.811738	0.007946	0.707084
-43.149867	-1.468837	1.816742	0.008014	0.707083
-42.999293	-1.493280	1.821747	0.007986	0.707088
-42.685424	-1.554373	1.826752	0.007927	0.707078
-43.109688	-1.612003	1.831757	0.008006	0.706811
-43.988656	-1.482890	1.836762	0.008169	0.706756
-44.106573	-1.464955	1.841766	0.008191	0.706751
-43.632106	-1.544492	1.846771	0.008102	0.706761
-43.934194	-1.495437	1.851776	0.008158	0.706752
-44.114135	-1.459996	1.856781	0.008191	0.706759
-43.616597	-1.550446	1.861786	0.008099	0.706756
-43.791350	-1.619820	1.866790	0.008131	0.706555
-44.912728	-1.469389	1.871795	0.008339	0.706456
-44.730482	-1.507210	1.876800	0.008305	0.706446
-44.632300	-1.522551	1.881805	0.008287	0.706451
-44.955135	-1.464746	1.886810	0.008346	0.706452
-44.938844	-1.471431	1.891814	0.008343	0.706444
-44.498841	-1.545140	1.896819	0.008261	0.706454
-44.791056	-1.577415	1.901824	0.008315	0.706285
-45.993217	-1.439736	1.906829	0.008539	0.706132
-45.181141	-1.585909	1.911834	0.008387	0.706130
-45.328612	-1.562547	1.916838	0.008414	0.706124
-45.535104	-1.520627	1.921843	0.008453	0.706135
-45.687744	-1.498905	1.926848	0.008481	0.706124
-45.547238	-1.521792	1.931853	0.008454	0.706129
-45.536319	-1.606666	1.936858	0.008452	0.705963
-46.807854	-1.429377	1.941862	0.008689	0.705864
-46.037326	-1.562984	1.946867	0.008545	0.705872
-46.030937	-1.570657	1.951872	0.008543	0.705860
-46.492504	-1.485518	1.956877	0.008629	0.705866
-46.188426	-1.539933	1.961882	0.008572	0.705866
-46.255003	-1.535335	1.966886	0.008584	0.705852
-46.950349	-1.569334	1.971891	0.008714	0.705535
-47.292472	-1.512780	1.976896	0.008777	0.705526
-47.423510	-1.487650	1.981901	0.008801	0.705530
-47.178638	-1.530775	1.986906	0.008755	0.705532
-47.535889	-1.468188	1.991910	0.008822	0.705530
-47.444958	-1.479642	1.996915	0.008804	0.705540
-47.374475	-1.558227	2.001920	0.008791	0.705408

-48.247744	-1.497618	2.011917	0.008953	0.705217
-48.086475	-1.526628	2.021914	0.008923	0.705218
-47.920121	-1.557360	2.031910	0.008891	0.705217
-48.453262	-1.461878	2.041907	0.008990	0.705218
-47.949813	-1.553093	2.051904	0.008896	0.705217
-48.215842	-1.506937	2.061901	0.008945	0.705215
-48.295716	-1.492027	2.071898	0.008959	0.705217
-48.140423	-1.519661	2.081894	0.008929	0.705218
-48.329360	-1.487521	2.091891	0.008964	0.705216
-48.198073	-1.505480	2.101888	0.008939	0.705228
-47.302716	-1.515558	2.111885	0.008772	0.705530
-47.304551	-1.513200	2.121882	0.008772	0.705535
-47.176252	-1.536604	2.131878	0.008747	0.705535
-47.403033	-1.497757	2.141875	0.008789	0.705533
-47.194880	-1.535397	2.151872	0.008750	0.705533
-47.262634	-1.523579	2.161869	0.008762	0.705533
-46.806122	-1.494284	2.171866	0.008676	0.705757
-46.172154	-1.553437	2.181862	0.008558	0.705866
-46.575691	-1.481139	2.191859	0.008632	0.705868
-46.323381	-1.527893	2.201856	0.008585	0.705866
-46.316657	-1.506310	2.211853	0.008583	0.705912
-45.443250	-1.553482	2.221850	0.008420	0.706132
-45.555478	-1.533698	2.231846	0.008440	0.706132
-45.903389	-1.471861	2.241843	0.008505	0.706133
-45.597845	-1.479201	2.251840	0.008447	0.706228
-45.008688	-1.476505	2.261837	0.008337	0.706446
-44.769764	-1.519122	2.271834	0.008292	0.706447
-44.889158	-1.498216	2.281830	0.008314	0.706447
-44.211151	-1.491481	2.291827	0.008187	0.706704
-43.998428	-1.506316	2.301824	0.008147	0.706752
-43.939327	-1.517189	2.311821	0.008135	0.706752
-43.760484	-1.506489	2.321818	0.008102	0.706839
-42.924998	-1.533157	2.331814	0.007946	0.707085
-42.857247	-1.544949	2.341811	0.007932	0.707087
-43.132137	-1.498429	2.351808	0.007983	0.707083
-42.829990	-1.471220	2.361805	0.007926	0.707246
-41.872976	-1.575438	2.371802	0.007748	0.707381
-42.175357	-1.521605	2.381798	0.007803	0.707382
-42.159828	-1.525451	2.391795	0.007800	0.707380
-41.577139	-1.475360	2.401792	0.007691	0.707690
-41.514410	-1.483527	2.411789	0.007679	0.707697
-41.197607	-1.538384	2.421786	0.007619	0.707701
-40.861709	-1.503006	2.431782	0.007556	0.707893
-40.509921	-1.506684	2.441779	0.007490	0.708013
-40.547410	-1.500301	2.451776	0.007497	0.708013
-40.450559	-1.499541	2.461773	0.007478	0.708050
-39.491409	-1.519978	2.471770	0.007299	0.708353
-39.664787	-1.490506	2.481766	0.007331	0.708351
-39.427857	-1.532292	2.491763	0.007286	0.708353
-39.231234	-1.481553	2.501760	0.007249	0.708526
-38.731052	-1.512753	2.511757	0.007155	0.708643
-38.576464	-1.540993	2.521754	0.007126	0.708643
-38.698192	-1.507033	2.531750	0.007148	0.708668
-37.968360	-1.492153	2.541747	0.007012	0.708959
-37.978686	-1.490533	2.551744	0.007013	0.708960
-37.739530	-1.532869	2.561741	0.006968	0.708961
-37.390546	-1.495305	2.571738	0.006903	0.709162
-37.162929	-1.482438	2.581734	0.006860	0.709270
-37.021928	-1.507436	2.591731	0.006833	0.709271
-37.078045	-1.445868	2.601728	0.006843	0.709376
-35.996839	-1.527562	2.611725	0.006641	0.709599
-35.848079	-1.553122	2.621722	0.006613	0.709601
-36.000242	-1.527435	2.631718	0.006641	0.709600
-35.721089	-1.475491	2.641715	0.006588	0.709804
-35.441901	-1.480987	2.651712	0.006536	0.709893
-35.292337	-1.507353	2.661709	0.006507	0.709895
-35.131057	-1.473886	2.671706	0.006477	0.710020
-34.301769	-1.521286	2.681702	0.006322	0.710222
-34.234068	-1.535526	2.691699	0.006309	0.710219
-34.562874	-1.478010	2.701696	0.006369	0.710217
-33.753104	-1.486301	2.711693	0.006218	0.710490
-33.678303	-1.478410	2.721690	0.006204	0.710534
-33.564757	-1.498708	2.731686	0.006182	0.710534
-33.073347	-1.502448	2.741683	0.006090	0.710703
-32.603116	-1.504193	2.751680	0.006002	0.710868
-32.552077	-1.514251	2.761677	0.005992	0.710867
-32.722243	-1.482580	2.771674	0.006023	0.710870
-32.243030	-1.449959	2.781670	0.005933	0.711107
-31.901521	-1.495959	2.791667	0.005869	0.711138
-32.100196	-1.459482	2.801664	0.005906	0.711141
-31.330697	-1.487001	2.811661	0.005762	0.711360
-31.206488	-1.460424	2.821658	0.005738	0.711459
-31.114696	-1.478488	2.831654	0.005721	0.711456
-30.656536	-1.503340	2.841651	0.005635	0.711570
-30.086472	-1.509201	2.851648	0.005528	0.711762
-30.052730	-1.516491	2.861645	0.005521	0.711761
-30.209249	-1.487604	2.871642	0.005550	0.711764
-29.435334	-1.494238	2.881638	0.005405	0.712026
-29.431426	-1.462724	2.891635	0.005404	0.712091
-29.416354	-1.467197	2.901632	0.005401	0.712089
-29.056270	-1.462709	2.911629	0.005333	0.712227
-28.407547	-1.497162	2.921626	0.005212	0.712389
-28.228964	-1.530143	2.931622	0.005178	0.712388
-28.414225	-1.497665	2.941619	0.005212	0.712388
-28.004577	-1.417876	2.951616	0.005135	0.712693
-27.632233	-1.477413	2.961613	0.005065	0.712708
-27.355294	-1.524817	2.971610	0.005013	0.712713
-27.272948	-1.447692	2.981606	0.004998	0.712896
-26.879892	-1.455198	2.991603	0.004924	0.713022
-26.774972	-1.474503	3.001600	0.004904	0.713021
-26.568989	-1.470738	3.011597	0.004865	0.713103
-25.906512	-1.460897	3.021594	0.004741	0.713358
-25.495999	-1.534767	3.031590	0.004664	0.713358
-25.885755	-1.466564	3.041587	0.004736	0.713356
-25.257086	-1.482405	3.051584	0.004619	0.713549
-24.898730	-1.497422	3.061581	0.004551	0.713647
-24.873335	-1.500475	3.071578	0.004546	0.713651
-24.750485	-1.509688	3.081574	0.004523	0.713677
-24.190419	-1.463124	3.091571	0.004418	0.713969
-23.996112	-1.498511	3.101568	0.004381	0.713968
-24.272746	-1.450662	3.111565	0.004432	0.713966
-23.729582	-1.441738	3.121562	0.004331	0.714177
-23.007800	-1.519527	3.131558	0.004196	0.714279
-23.442889	-1.444394	3.141555	0.004276	0.714275
-23.152381	-1.451949	3.151552	0.004222	0.714364
-22.132449	-1.510030	3.161549	0.004031	0.714611
-22.112371	-1.512919	3.171546	0.004027	0.714613
-22.291234	-1.481783	3.181542	0.004060	0.714613
-21.892030	-1.452304	3.191539	0.003985	0.714813
-21.432727	-1.486467	3.201536	0.003899	0.714909
-21.570070	-1.462532	3.211533	0.003924	0.714909
-21.350242	-1.466156	3.221530	0.003882	0.714980
-20.540983	-1.483079	3.231526	0.003731	0.715234
-20.511603	-1.488609	3.241523	0.003725	0.715234
-20.410721	-1.507074	3.251520	0.003706	0.715234
-20.045230	-1.466331	3.261517	0.003637	0.715445
-19.614894	-1.491856	3.271514	0.003557	0.715547
-19.600514	-1.494202	3.281510	0.003553	0.715549
-19.665818	-1.463157	3.291507	0.003565	0.715588
-18.805926	-1.468514	3.301504	0.003404	0.715882
-18.717296	-1.484401	3.311501	0.003387	0.715883
-18.606393	-1.502916	3.321498	0.003366	0.715886
-18.303032	-1.490957	3.331494	0.003309	0.716018
-18.031607	-1.480633	3.341491	0.003258	0.716135
-17.842675	-1.516557	3.351488	0.003223	0.716132
-18.010337	-1.472429	3.361485	0.003253	0.716161
-17.228266	-1.465806	3.371482	0.003107	0.716451
-17.007298	-1.503845	3.381478	0.003065	0.716455
-17.278824	-1.457431	3.391475	0.003115	0.716452
-16.334066	-1.504636	3.401472	0.002939	0.716693
-16.164991	-1.502910	3.411469	0.002907	0.716757
-15.684041	-1.588007	3.421466	0.002817	0.716759
-15.871933	-1.555584	3.431462	0.002852	0.716758
-15.188040	-1.529639	3.441459	0.002724	0.717051
-14.811708	-1.580141	3.451456	0.002653	0.717085
-14.991381	-1.548748	3.461453	0.002686	0.717084
-14.738690	-1.591447	3.471450	0.002638	0.717090
-14.457168	-1.507508	3.481446	0.002585	0.717356
-13.928869	-1.588982	3.491443	0.002487	0.717382
-14.103911	-1.559205	3.501440	0.002519	0.717380
-13.917617	-1.568417	3.511437	0.002484	0.717429
-12.980227	-1.595222	3.521434	0.002308	0.717707
-13.011552	-1.589147	3.531430	0.002314	0.717709
-13.037978	-1.584775	3.541427	0.002318	0.717709
-13.017393	-1.527168	3.551424	0.002314	0.717831
-12.100411	-1.597051	3.561421	0.002143	0.718017
-11.902195	-1.630594	3.571418	0.002105	0.718021
-12.102072	-1.596713	3.581414	0.002142	0.718019
-11.820102	-1.566206	3.591411	0.002089	0.718179
-11.014110	-1.621295	3.601408	0.001938	0.718355
-11.106816	-1.604841	3.611405	0.001955	0.718356
-10.897531	-1.641343	3.621402	0.001916	0.718358
-10.824980	-1.572506	3.631398	0.001901	0.718521
-10.055828	-1.646050	3.641395	0.001758	0.718647
-10.280190	-1.607296	3.651392	0.001799	0.718645
-10.387852	-1.589367	3.661389	0.001819	0.718644
-9.441578	-1.607864	3.671386	0.001642	0.718941
-9.344431	-1.613062	3.681382	0.001623	0.718966
-9.201466	-1.639849	3.691379	0.001596	0.718964
-9.376855	-1.579078	3.701376	0.001628	0.719023
-8.271001	-1.651946	3.711373	0.001422	0.719269
-8.396187	-1.629192	3.721370	0.001445	0.719271
-8.543643	-1.601879	3.731366	0.001472	0.719274
-8.010444	-1.604069	3.741363	0.001372	0.719458
-7.773322	-1.573923	3.751360	0.001327	0.719602
-7.436253	-1.633296	3.761357	0.001264	0.719604
-7.439641	-1.631798	3.771354	0.001264	0.719607
-6.730192	-1.610989	3.781350	0.001131	0.719898
-6.580332	-1.636425	3.791347	0.001103	0.719901
-6.690656	-1.617191	3.801344	0.001123	0.719901
-6.569570	-1.588828	3.811341	0.001100	0.720000
-5.625299	-1.643008	3.821338	0.000924	0.720226
-5.768986	-1.615770	3.831334	0.000950	0.720230
-5.767451	-1.617965	3.841331	0.000949	0.720227
-5.272403	-1.576583	3.851328	0.000856	0.720483
-4.762918	-1.637830	3.861325	0.000761	0.720542
-4.991340	-1.596455	3.871322	0.000803	0.720545
-4.945440	-1.547427	3.881318	0.000794	0.720658
-3.791336	-1.638379	3.891315	0.000578	0.720885
-3.960503	-1.609622	3.901312	0.000609	0.720883
-3.917926	-1.618054	3.911309	0.000601	0.720882
-3.636604	-1.581043	3.921306	0.000548	0.721055
-3.448077	-1.578908	3.931302	0.000512	0.721126
-3.349597	-1.596381	3.941299	0.000494	0.721127
-3.130707	-1.558714	3.951296	0.000452	0.721279
-2.813263	-1.533728	3.961293	0.000393	0.721440
-2.475625	-1.592396	3.971290	0.000329	0.721444
-2.739711	-1.484952	3.981286	0.000378	0.721563
-2.089747	-1.505739	3.991283	0.000256	0.721751
-1.863027	-1.547160	4.001280	0.000214	0.721750
-1.948693	-1.447672	4.011277	0.000229	0.721916
-1.078512	-1.518642	4.021274	0.000067	0.722082
-1.795904	-1.392032	4.031270	0.000200	0.722081
-1.534748	-1.326836	4.041267	0.000150	0.722301
-1.002493	-1.384843	4.051264	0.000051	0.722374
-1.398242	-1.269087	4.061261	0.000124	0.722464
-1.035536	-1.214383	4.071258	0.000056	0.722699
-1.107689	-1.176500	4.081254	0.000069	0.722749
-0.744226	-1.107737	4.091251	0.000000	0.723012
-0.608812	-1.120825	4.101248	-0.000025	0.723035
-0.569399	-0.970513	4.111245	-0.000033	0.723344
-0.524078	-0.950493	4.121242	-0.000042	0.723400
-0.448067	-0.839439	4.131238	-0.000057	0.723645
-0.647317	-0.731472	4.141235	-0.000020	0.723788
-0.930572	-0.594291	4.151232	0.000032	0.723959
-0.636412	-0.492924	4.161229	-0.000024	0.724261
-0.245809	-0.473181	4.171226	-0.000097	0.724437
-0.297683	-0.369370	4.181222	-0.000088	0.724623
-0.164317	-0.253773	4.191219	-0.000113	0.724897
-0.367196	-0.101480	4.201216	-0.000076	0.725125
-0.205547	-0.012287	4.211213	-0.000107	0.725357
0.000066	0.076396	4.221210	-0.000146	0.725603
0.000000	0.271736	4.231206	-0.000146	0.725985

0.066687	0.878996	4.236211	-0.000159	0.727194
0.520465	2.072730	4.241216	-0.000245	0.729676
0.807664	3.894249	4.246221	-0.000300	0.733306
1.030414	6.269860	4.251226	-0.000343	0.737963
1.575323	9.109372	4.256230	-0.000447	0.743584
2.054701	12.451962	4.261235	-0.000538	0.750093
2.332269	16.272103	4.266240	-0.000593	0.757373
2.890949	20.455839	4.271245	-0.000700	0.765350
3.186411	25.089960	4.276250	-0.000758	0.773985
3.646125	30.060130	4.281254	-0.000847	0.783186
4.104963	35.379983	4.286259	-0.000936	0.792904
4.917642	40.952439	4.291264	-0.001092	0.803062
5.508039	46.884917	4.296269	-0.001206	0.813652
5.849119	53.121609	4.301274	-0.001273	0.824552
6.351918	59.626689	4.306278	-0.001372	0.835814
6.975325	66.303742	4.311283	-0.001492	0.847250
7.335706	73.250927	4.316288	-0.001564	0.858902
7.820266	80.388087	4.321293	-0.001659	0.870743
8.435486	87.667763	4.326298	-0.001779	0.882691
9.013204	95.147643	4.331302	-0.001892	0.894786
9.378331	102.810125	4.336307	-0.001965	0.906946
9.996329	110.577910	4.341312	-0.002085	0.919176
10.743550	118.449786	4.346317	-0.002230	0.931438
11.048764	126.494217	4.351322	-0.002292	0.943683
11.896040	134.572570	4.356326	-0.002455	0.955962
12.436887	142.772777	4.361331	-0.002562	0.968184
12.889085	151.074242	4.366336	-0.002651	0.980379
13.496049	159.448873	4.371341	-0.002770	0.992566
14.458977	167.776296	4.376346	-0.002955	1.004625
15.225767	176.208773	4.381350	-0.003104	1.016640
15.419772	184.774609	4.386355	-0.003146	1.028561
16.294196	193.249834	4.391360	-0.003314	1.040382
16.984352	201.804124	4.396365	-0.003449	1.052134
17.517963	210.397976	4.401370	-0.003554	1.063772
18.151135	219.023177	4.406374	-0.003678	1.075348
18.766891	227.630093	4.411379	-0.003798	1.086772
18.804369	236.348726	4.416384	-0.003811	1.098093
19.512527	244.963805	4.421389	-0.003949	1.109313
20.007041	253.596815	4.426394	-0.004047	1.120397
20.619236	262.219890	4.431398	-0.004167	1.131385
21.051103	270.869436	4.436403	-0.004253	1.142261
21.439816	279.545068	4.441408	-0.004331	1.153057
21.911757	288.175066	4.446413	-0.004425	1.163715
22.508843	296.756698	4.451418	-0.004542	1.174243
23.064874	305.346295	4.456422	-0.004651	1.184679
23.572552	313.949411	4.461427	-0.004752	1.195029
24.002658	322.516683	4.466432	-0.004838	1.205233
24.455036	331.116609	4.471437	-0.004928	1.215393
24.880176	339.678384	4.476442	-0.005013	1.225419
25.554795	348.221906	4.481446	-0.005144	1.235392
26.220648	356.713994	4.486451	-0.005274	1.245223
26.510441	365.272996	4.491456	-0.005334	1.254982
27.235579	373.744786	4.496461	-0.005475	1.264649
27.345788	382.309935	4.501466	-0.005501	1.274231
27.692047	390.806690	4.506470	-0.005571	1.283710
28.238026	399.271574	4.511475	-0.005679	1.293122
28.882324	407.700747	4.516480	-0.005804	1.302444
29.385593	416.242371	4.521485	-0.005904	1.311795
29.525075	424.754188	4.526490	-0.005936	1.320983
30.366204	433.106751	4.531494	-0.006098	1.330062
30.636032	441.542887	4.536499	-0.006154	1.339067
31.006141	449.944330	4.541504	-0.006229	1.347993
31.427444	458.357373	4.546509	-0.006313	1.356881
31.664817	466.739645	4.551514	-0.006363	1.365648
32.077700	475.126458	4.556518	-0.006445	1.374393
32.476265	483.490113	4.561523	-0.006525	1.383056
32.760842	491.874015	4.566528	-0.006584	1.391667
33.282433	500.200415	4.571533	-0.006687	1.400206
33.677835	508.521801	4.576538	-0.006766	1.408667
34.176992	516.847216	4.581542	-0.006865	1.417099
34.592871	525.170504	4.586547	-0.006948	1.425464
34.812974	533.528126	4.591552	-0.006995	1.433783
35.405035	541.801412	4.596557	-0.007110	1.442031
35.596310	550.135573	4.601562	-0.007152	1.450227
36.064331	558.437348	4.606566	-0.007245	1.458389
36.582332	566.711733	4.611571	-0.007347	1.466488
37.117352	575.036502	4.616576	-0.007452	1.474592
37.422805	583.332910	4.621581	-0.007514	1.482590
37.637453	591.618174	4.626586	-0.007560	1.490519
38.188433	599.874302	4.631590	-0.007668	1.498431
38.436646	608.155382	4.636595	-0.007720	1.506278
38.555578	616.465243	4.641600	-0.007748	1.514091
39.181155	624.665173	4.646605	-0.007870	1.521839
39.715260	632.887555	4.651610	-0.007975	1.529554
39.951579	641.178016	4.656614	-0.008025	1.537249
40.394472	649.401113	4.661619	-0.008113	1.544874
40.595726	657.687653	4.666624	-0.008156	1.552483
40.909791	665.934506	4.671629	-0.008220	1.560036
41.003955	674.192008	4.676634	-0.008243	1.567530
41.424797	682.412004	4.681638	-0.008327	1.575002
41.677381	690.642042	4.686643	-0.008380	1.582423
41.928111	698.875806	4.691648	-0.008432	1.589813
42.306430	707.098495	4.696653	-0.008508	1.597176
42.608172	715.296776	4.701658	-0.008570	1.604473
43.037472	723.501663	4.706662	-0.008656	1.611761
43.565178	731.690460	4.711667	-0.008760	1.619016
43.769886	739.909892	4.716672	-0.008803	1.626220
44.235303	748.165796	4.721677	-0.008896	1.633459
44.426807	756.359778	4.726682	-0.008937	1.640575
45.112921	764.490598	4.731686	-0.009070	1.647674
45.466125	772.698433	4.736691	-0.009142	1.654763
45.390917	780.929803	4.741696	-0.009133	1.661784
45.815117	789.103397	4.746701	-0.009218	1.668793
46.042058	797.305839	4.751706	-0.009266	1.675771
46.483532	805.452577	4.756710	-0.009353	1.682701
47.129611	813.590055	4.761715	-0.009479	1.689622
47.546971	821.764296	4.766720	-0.009562	1.696515
47.638782	829.994544	4.771725	-0.009585	1.703384
47.795402	838.197045	4.776730	-0.009620	1.710211
48.171202	846.371339	4.781734	-0.009696	1.717016
48.560760	854.515527	4.786739	-0.009774	1.723771
48.607907	862.708866	4.791744	-0.009788	1.730496
49.135999	870.861226	4.796749	-0.009892	1.737222
49.625450	878.985110	4.801754	-0.009989	1.743895
50.162852	887.131013	4.806758	-0.010094	1.750566
50.649222	895.289227	4.811763	-0.010190	1.757214
51.094233	903.417265	4.816768	-0.010279	1.763809
51.641032	911.565408	4.821773	-0.010386	1.770407
51.793483	919.767313	4.826778	-0.010420	1.776974
52.127935	927.923683	4.831782	-0.010488	1.783504
52.571301	936.096947	4.836787	-0.010576	1.790036
52.607741	944.326395	4.841792	-0.010589	1.796539
52.847240	952.459680	4.846797	-0.010639	1.802968
53.041693	960.597909	4.851802	-0.010680	1.809372
53.230212	968.756898	4.856806	-0.010721	1.815769
53.621773	976.882617	4.861811	-0.010800	1.822142
53.977450	985.002399	4.866816	-0.010871	1.828484
54.513119	993.136188	4.871821	-0.010977	1.834835
54.786363	1001.261688	4.876826	-0.011033	1.841128
54.955629	1009.414120	4.881830	-0.011070	1.847407
55.405126	1017.562764	4.886835	-0.011159	1.853695
55.681680	1025.679874	4.891840	-0.011217	1.859917
56.142917	1033.808970	4.896845	-0.011308	1.866149
56.583105	1041.952597	4.901850	-0.011395	1.872369
56.980970	1050.079235	4.906854	-0.011475	1.878550
57.005388	1058.236703	4.911859	-0.011485	1.884691
57.361353	1066.347058	4.916864	-0.011557	1.890815
57.733689	1074.477173	4.921869	-0.011632	1.896936
57.844852	1082.607642	4.926874	-0.011658	1.903007
58.231475	1090.716367	4.931878	-0.011736	1.909074
58.790211	1098.815079	4.936883	-0.011845	1.915134
58.975873	1106.942526	4.941888	-0.011885	1.921154
59.131634	1115.091243	4.946893	-0.011920	1.927167
59.553475	1123.201600	4.951898	-0.012004	1.933163
59.961807	1131.305565	4.956902	-0.012086	1.939134
60.195905	1139.430836	4.961907	-0.012135	1.945083
60.558718	1147.562747	4.966912	-0.012208	1.951032
60.775438	1155.727476	4.971917	-0.012254	1.956972
60.959444	1163.815418	4.976922	-0.012294	1.962834
61.320675	1171.899700	4.981926	-0.012366	1.968695
61.888134	1179.993065	4.986931	-0.012478	1.974567
62.150897	1188.094446	4.991936	-0.012532	1.980395
62.510042	1196.196600	4.996941	-0.012604	1.986217
62.915152	1204.320844	5.001946	-0.012685	1.992042
63.096750	1212.441846	5.006950	-0.012725	1.997824
63.472317	1220.528168	5.011955	-0.012800	2.003585
63.666649	1228.643233	5.016960	-0.012842	2.009331
64.035992	1236.762036	5.021965	-0.012916	2.015082
64.084411	1244.879127	5.026970	-0.012931	2.020781
64.279128	1252.975708	5.031974	-0.012973	2.026465
64.780312	1261.083878	5.036979	-0.013072	2.032173
64.978138	1269.190474	5.041984	-0.013114	2.037832
65.134957	1277.296969	5.046989	-0.013149	2.043471
65.563216	1285.369894	5.051994	-0.013234	2.049100
65.963301	1293.463163	5.056998	-0.013314	2.054723
66.483593	1301.532946	5.062003	-0.013416	2.060328
70.627409	1309.114362	5.067008	-0.014193	2.065945
71.691597	1317.267084	5.072013	-0.014397	2.071629
72.076006	1325.463811	5.077018	-0.014474	2.077260
72.476916	1333.624188	5.082022	-0.014554	2.082852
72.630040	1341.828345	5.087027	-0.014588	2.088435
72.764413	1350.002578	5.092032	-0.014619	2.093980
72.931886	1358.152818	5.097037	-0.014656	2.099498
73.263997	1366.253912	5.102042	-0.014723	2.104984
73.658521	1374.371349	5.107046	-0.014802	2.110473
73.885079	1382.555034	5.112051	-0.014850	2.115976
74.168001	1390.606074	5.117056	-0.014908	2.121381
74.562171	1398.688137	5.122061	-0.014987	2.126804
74.752446	1406.801886	5.127066	-0.015028	2.132214
74.949595	1414.899815	5.132070	-0.015070	2.137601
75.515116	1422.936671	5.137075	-0.015181	2.142969
75.779620	1431.025619	5.142080	-0.015236	2.148329
75.982702	1439.162775	5.147085	-0.015279	2.153702
76.539949	1447.194580	5.152090	-0.015388	2.159025
77.137050	1455.234032	5.157094	-0.015505	2.164344
77.535935	1463.323868	5.162099	-0.015585	2.169664
77.621282	1471.459274	5.167104	-0.015606	2.174971
77.865194	1479.559161	5.172109	-0.015657	2.180258
78.156088	1487.640173	5.177114	-0.015717	2.185523
78.616710	1495.733297	5.182118	-0.015808	2.190799
78.924580	1503.848026	5.187123	-0.015871	2.196062
79.231873	1511.889782	5.192128	-0.015934	2.201266
79.510906	1519.987166	5.197133	-0.015991	2.206490
79.717018	1528.071045	5.202138	-0.016035	2.211687
80.107523	1536.131779	5.207142	-0.016114	2.216873
80.612073	1544.202776	5.212147	-0.016213	2.222064
80.732212	1552.292890	5.217152	-0.016241	2.227221
81.248039	1560.382879	5.222157	-0.016342	2.232400
81.303105	1568.479721	5.227162	-0.016358	2.237531
81.498912	1576.541894	5.232166	-0.016400	2.242641
81.763458	1584.631868	5.237171	-0.016455	2.247763
82.223579	1592.690388	5.242176	-0.016546	2.252870
82.791483	1600.725640	5.247181	-0.016657	2.257960
83.196057	1608.782402	5.252186	-0.016738	2.263038
83.752453	1616.857272	5.257190	-0.016847	2.268129
84.208820	1625.009693	5.262195	-0.016938	2.273249
84.424306	1633.066839	5.267200	-0.016984	2.278276
84.994693	1641.088900	5.272205	-0.017095	2.283301
85.188277	1649.174447	5.277210	-0.017137	2.288323
85.600947	1657.245705	5.282214	-0.017219	2.293342
85.823769	1665.345841	5.287219	-0.017266	2.298353
86.110827	1673.394259	5.292224	-0.017325	2.303326
86.437357	1681.473463	5.297229	-0.017392	2.308311
86.756162	1689.558920	5.302234	-0.017456	2.313288
87.295341	1697.586358	5.307238	-0.017562	2.318237
87.682802	1705.663327	5.312243	-0.017640	2.323193
88.008690	1713.721774	5.317248	-0.017706	2.328122
88.495306	1721.783632	5.322253	-0.017802	2.333056
88.988528	1729.848072	5.327258	-0.017900	2.337981
89.107145	1737.937287	5.332262	-0.017927	2.342880
89.421266	1746.028683	5.337267	-0.017991	2.347787
89.607861	1754.136579	5.342272	-0.018032	2.352682
89.897200	1762.212493	5.347277	-0.018091	2.357556
90.006345	1770.274121	5.352282	-0.018117	2.362398
90.489319	1778.292844	5.357286	-0.018212	2.367233
90.785938	1786.392120	5.362291	-0.018273	2.372092
90.996845	1794.455205	5.367296	-0.018318	2.376912
91.568772	1802.471384	5.372301	-0.018430	2.381724
92.089463	1810.522882	5.377306	-0.018532	2.386542
92.162851	1818.631856	5.382310	-0.018551	2.391350
92.697034	1826.701992	5.387315	-0.018656	2.396161
93.018084	1834.737391	5.392320	-0.018722	2.400925
93.459706	1842.794948	5.397325	-0.018809	2.405702
93.595843	1850.886045	5.402330	-0.018840	2.410465
93.901670	1858.966979	5.407334	-0.018903	2.415226
94.408242	1867.013945	5.412339	-0.019003	2.419973
94.754783	1875.049275	5.417344	-0.019073	2.424692
95.082145	1883.139496	5.422349	-0.019139	2.429432
95.506783	1891.277765	5.427354	-0.019224	2.434198
95.761017	1899.304806	5.432358	-0.019276	2.438877
96.158731	1907.334213	5.437363	-0.019356	2.443559
96.777989	1915.332604	5.442368	-0.019477	2.448232
97.382962	1923.400269	5.447373	-0.019595	2.452934
97.685952	1931.464529	5.452378	-0.019657	2.457602
97.969787	1939.520472	5.457382	-0.019715	2.462255
98.360813	1947.585737	5.462387	-0.019794	2.466912
98.795937	1955.652841	5.467392	-0.019880	2.471566
99.156033	1963.717059	5.472397	-0.019953	2.476202
99.617789	1971.754110	5.477402	-0.020044	2.480823
99.917974	1979.803838	5.482406	-0.020106	2.485430
100.447434	1987.872228	5.487411	-0.020210	2.490055
100.782394	1995.945354	5.492416	-0.020278	2.494661
101.559637	2003.957958	5.497421	-0.020428	2.499256
101.946226	2012.026011	5.502426	-0.020505	2.503845
102.362424	2020.088690	5.507430	-0.020588	2.508425
102.885087	2028.194009	5.512435	-0.020691	2.513028
102.884510	2036.275322	5.517440	-0.020697	2.517571
103.381147	2044.297704	5.522445	-0.020795	2.522109
104.047059	2052.329348	5.527450	-0.020924	2.526656
104.124433	2060.422383	5.532454	-0.020944	2.531187
104.399848	2068.517002	5.537459	-0.021001	2.535724
104.804808	2076.534628	5.542464	-0.021082	2.540220
105.235242	2084.579488	5.547469	-0.021167	2.544725
105.591016	2092.645274	5.552474	-0.021239	2.549228
106.127108	2100.693925	5.557478	-0.021344	2.553726
106.441873	2108.773578	5.562483	-0.021408	2.558218
106.630670	2116.806336	5.567488	-0.021449	2.562667
106.940821	2124.871574	5.572493	-0.021512	2.567135
107.427722	2132.910027	5.577498	-0.021609	2.571592
107.843886	2140.963966	5.582502	-0.021692	2.576045
108.296359	2149.018138	5.587507	-0.021781	2.580493
108.538524	2157.057817	5.592512	-0.021832	2.584911
108.853056	2165.125491	5.597517	-0.021896	2.589342
109.201748	2173.384476	5.602522	-0.021967	2.593872
109.479855	2181.376046	5.607526	-0.022024	2.598243
109.962090	2189.362966	5.612531	-0.022119	2.602618
110.152031	2197.379600	5.617536	-0.022160	2.606982
110.572453	2205.414280	5.622541	-0.022244	2.611364
111.154478	2213.449582	5.627546	-0.022358	2.615750
111.429580	2221.469088	5.632550	-0.022414	2.620099
111.819674	2229.508431	5.637555	-0.022492	2.624460
112.321747	2237.549869	5.642560	-0.022591	2.628821
112.810114	2245.611025	5.647565	-0.022688	2.633185
112.870845	2253.705923	5.652570	-0.022705	2.637532
113.191855	2261.719192	5.657574	-0.022770	2.641844
113.742368	2269.760521	5.662579	-0.022878	2.646180
113.938845	2277.807275	5.667584	-0.022920	2.650488
114.353543	2285.871899	5.672589	-0.023003	2.654813
114.707521	2293.912131	5.677594	-0.023074	2.659114
115.081239	2301.937307	5.682598	-0.023149	2.663401
115.489280	2310.010346	5.687603	-0.023231	2.667709
115.932588	2318.067019	5.692608	-0.023319	2.672003
116.615435	2326.103105	5.697613	-0.023451	2.676295
116.949447	2334.132631	5.702618	-0.023519	2.680554
117.202664	2342.177203	5.707622	-0.023572	2.684809
117.724278	2350.223045	5.712627	-0.023674	2.689075
118.257236	2358.268711	5.717632	-0.023779	2.693334
118.411563	2366.370662	5.722637	-0.023813	2.697593
118.800019	2374.391711	5.727642	-0.023891	2.701817
119.377177	2382.406476	5.732646	-0.024004	2.706043
119.825920	2390.467467	5.737651	-0.024093	2.710278
120.077827	2398.534314	5.742656	-0.024146	2.714498
120.626821	2406.538135	5.747661	-0.024253	2.718696
121.038425	2414.599913	5.752666	-0.024335	2.722910
121.057258	2422.644695	5.757670	-0.024344	2.727083
121.544845	2430.719091	5.762675	-0.024441	2.731295
122.103515	2438.761548	5.767680	-0.024550	2.735488
122.088147	2446.824784	5.772685	-0.024553	2.739650
122.461052	2454.872530	5.777690	-0.024628	2.743821
122.789449	2462.919791	5.782694	-0.024695	2.747983
123.092366	2471.038385	5.787699	-0.024757	2.752174
123.323731	2479.106109	5.792704	-0.024805	2.756327
123.758411	2487.105539	5.797709	-0.024892	2.760452
124.199109	2495.088388	5.802714	-0.024979	2.764563
124.258679	2503.140863	5.807718	-0.024996	2.768680
124.713301	2511.202660	5.812723	-0.025086	2.772819
125.099733	2519.233200	5.817728	-0.025163	2.776932
125.229568	2527.296561	5.822733	-0.025193	2.781040
125.514967	2535.326755	5.827738	-0.025252	2.785134
125.867859	2543.340144	5.832742	-0.025323	2.789218
126.040060	2551.447531	5.837747	-0.025360	2.793333
126.203653	2559.477126	5.842752	-0.025396	2.797402
126.527984	2567.484463	5.847757	-0.025462	2.801463
126.928920	2575.513984	5.852762	-0.025542	2.805534
126.963767	2583.567771	5.857766	-0.025554	2.809590
127.444968	2591.625414	5.862771	-0.025649	2.813667
127.797501	2599.648162	5.867776	-0.025721	2.817714
128.179094	2607.679942	5.872781	-0.025797	2.821761
128.542526	2615.721180	5.877786	-0.025870	2.825806
129.089540	2623.744432	5.882790	-0.025978	2.829847
129.475275	2631.846689	5.887795	-0.026055	2.833911
129.501282	2639.900162	5.892800	-0.026065	2.837926
129.896054	2647.913118	5.897805	-0.026144	2.841935
130.375900	2655.946202	5.902810	-0.026239	2.845953
130.659126	2663.968465	5.907814	-0.026297	2.849949
130.944049	2672.052407	5.912819	-0.026356	2.853971
131.224727	2680.087774	5.917824	-0.026414	2.857962
131.545243	2688.122459	5.922829	-0.026479	2.861949
131.434916	2696.201146	5.927834	-0.026464	2.865929
131.994087	2704.186693	5.932838	-0.026573	2.869894
132.413198	2712.251998	5.937843	-0.026657	2.873885
132.554103	2720.288649	5.942848	-0.026689	2.877841
133.042682	2728.289346	5.947853	-0.026785	2.881794
133.504287	2736.313233	5.952858	-0.026877	2.885750
133.569568	2744.373334	5.957862	-0.026894	2.889697
134.089331	2752.424072	5.962867	-0.026997	2.893659
134.338786	2760.461679	5.967872	-0.027049	2.897594
134.830243	2768.497036	5.972877	-0.027146	2.901536
134.930303	2776.564367	5.977882	-0.027170	2.905467
135.149589	2784.602534	5.982886	-0.027216	2.909385
135.599823	2792.720230	5.987891	-0.027305	2.913348
135.853666	2800.739303	5.992896	-0.027358	2.917248
135.980451	2808.753495	5.997901	-0.027387	2.921133
136.209430	2816.787927	6.002906	-0.027435	2.925029
136.405473	2824.794081	6.007910	-0.027477	2.928903
136.644226	2832.850361	6.012915	-0.027527	2.932799
136.957757	2840.882087	6.017920	-0.027591	2.936682
137.233000	2848.902139	6.022925	-0.027648	2.940552
137.543128	2856.918063	6.027930	-0.027711	2.944417
137.878848	2864.953647	6.032934	-0.027779	2.948287
138.094312	2873.039732	6.037939	-0.027825	2.952170
138.135485	2881.120123	6.042944	-0.027838	2.956037
138.369905	2889.100684	6.047949	-0.027887	2.959860
138.834529	2897.104270	6.052954	-0.027979	2.963702
139.063685	2905.129346	6.057958	-0.028027	2.967536
139.379923	2913.199597	6.062963	-0.028092	2.971391
139.875954	2921.234314	6.067968	-0.028189	2.975234
140.106094	2929.255407	6.072973	-0.028238	2.979051
140.403397	2937.301515	6.077978	-0.028299	2.982879
140.417728	2945.348620	6.082982	-0.028307	2.986688
140.832413	2953.394566	6.087987	-0.028390	2.990512
141.003471	2961.476860	6.092992	-0.028427	2.994336
141.338269	2969.461477	6.097997	-0.028495	2.998117
141.882187	2977.493324	6.103002	-0.028601	3.001926
142.126265	2985.514124	6.108006	-0.028652	3.005710
142.365559	2993.558308	6.113011	-0.028702	3.009500
142.951153	3001.591718	6.118016	-0.028817	3.013297
143.385006	3009.606800	6.123021	-0.028903	3.017073
143.635434	3017.673383	6.128026	-0.028955	3.020859
143.700366	3025.683353	6.133030	-0.028973	3.024605
144.382972	3033.705851	6.138035	-0.029106	3.028383
144.642291	3041.780757	6.143040	-0.029159	3.032159
144.889160	3049.827573	6.148045	-0.029211	3.035917
145.277287	3057.822822	6.153050	-0.029289	3.039653
145.655182	3065.837247	6.158054	-0.029364	3.043393
145.831258	3073.922987	6.163059	-0.029403	3.047151
145.996485	3081.972045	6.168064	-0.029439	3.050888
146.282418	3090.010545	6.173069	-0.029498	3.054620
146.418937	3098.058149	6.178074	-0.029529	3.058346
146.617464	3106.072736	6.183078	-0.029571	3.062054
147.197512	3114.096757	6.188083	-0.029685	3.065780
147.520539	3122.106193	6.193088	-0.029750	3.069483
147.787997	3130.232362	6.198093	-0.029806	3.073232
148.146391	3138.268208	6.203098	-0.029878	3.076939
148.494279	3146.251668	6.208102	-0.029948	3.080618
148.997458	3154.227760	6.213107	-0.030047	3.084295
149.256675	3162.283359	6.218112	-0.030101	3.087994
149.518535	3170.317049	6.223117	-0.030155	3.091678
149.759473	3178.381730	6.228122	-0.030206	3.095370
150.022543	3186.388176	6.233126	-0.030260	3.099033
150.441818	3194.424920	6.238131	-0.030344	3.102712
150.653851	3202.477067	6.243136	-0.030389	3.106385
150.666649	3210.524391	6.248141	-0.030397	3.110042
151.329598	3218.560412	6.253146	-0.030525	3.113718
151.629710	3226.548663	6.258150	-0.030587	3.117353
152.020699	3234.605679	6.263155	-0.030665	3.121018
152.336406	3242.584502	6.268160	-0.030729	3.124640
152.575621	3250.647408	6.273165	-0.030779	3.128293
152.878417	3258.718435	6.278170	-0.030841	3.131947
152.904907	3266.772210	6.283174	-0.030852	3.135577
153.489530	3274.746427	6.288179	-0.030966	3.139192
153.957362	3282.776348	6.293184	-0.031059	3.142823
153.854528	3290.851535	6.298189	-0.031045	3.146445
154.269606	3298.890215	6.303194	-0.031128	3.150068
154.538818	3306.937960	6.308198	-0.031183	3.153685
154.746603	3314.972448	6.313203	-0.031228	3.157290
154.912469	3322.992348	6.318208	-0.031264	3.160882
155.332205	3330.961150	6.323213	-0.031348	3.164458
155.803281	3339.000060	6.328218	-0.031441	3.168063
155.929442	3347.061356	6.333222	-0.031470	3.171659
156.199274	3355.122935	6.338227	-0.031526	3.175257
156.406421	3363.141493	6.343232	-0.031570	3.178830
156.761351	3371.133881	6.348237	-0.031641	3.182393
157.080846	3379.183189	6.353242	-0.031706	3.185976
157.273562	3387.185437	6.358246	-0.031748	3.189528
157.776630	3395.245464	6.363251	-0.031847	3.193116
158.029522	3403.289160	6.368256	-0.031899	3.196681
158.318933	3411.299578	6.373261	-0.031959	3.200229
158.510412	3419.329742	6.378266	-0.032000	3.203778
158.690341	3427.347311	6.383270	-0.032039	3.207317
159.366618	3435.381616	6.388275	-0.032170	3.210880
159.648401	3443.411908	6.393280	-0.032228	3.214420
159.752302	3451.467224	6.398285	-0.032253	3.217961
160.140347	3459.504795	6.403290	-0.032331	3.221501
160.376189	3467.502192	6.408294	-0.032380	3.225013
160.675250	3475.581058	6.413299	-0.032441	3.228560
160.722561	3483.651709	6.418304	-0.032456	3.232089
161.002451	3491.706698	6.423309	-0.032513	3.235617
161.306198	3499.696775	6.428314	-0.032575	3.239114
161.537071	3507.688055	6.433318	-0.032624	3.242604
161.855751	3515.704352	6.438323	-0.032689	3.246105
162.151066	3523.697127	6.443328	-0.032749	3.249591
162.471808	3531.771836	6.448333	-0.032814	3.253110
162.782360	3539.812456	6.453338	-0.032878	3.256610
163.128142	3547.791602	6.458342	-0.032947	3.260081
163.331301	3555.826404	6.463347	-0.032991	3.263566
163.418982	3563.879004	6.468352	-0.033013	3.267051
163.810549	3571.920513	6.473357	-0.033091	3.270539
163.960580	3580.003634	6.478362	-0.033125	3.274032
164.045004	3587.994866	6.483366	-0.033146	3.277479
164.355470	3596.019079	6.488371	-0.033209	3.280945
164.870258	3603.978992	6.493376	-0.033310	3.284388
164.986227	3612.040922	6.498381	-0.033337	3.287856
165.149538	3620.128278	6.503386	-0.033373	3.291333
165.471649	3628.129857	6.508390	-0.033439	3.294775
165.723768	3636.154991	6.513395	-0.033491	3.298221
165.868863	3644.196024	6.518400	-0.033524	3.301666
166.089287	3652.189836	6.523405	-0.033570	3.305090
166.546852	3660.256566	6.528410	-0.033661	3.308551
166.572242	3668.310280	6.533414	-0.033671	3.311986
166.819357	3676.365195	6.538419	-0.033723	3.315427
167.164141	3684.318666	6.543424	-0.033792	3.318824
167.314076	3692.346882	6.548429	-0.033826	3.322242
167.493052	3700.382361	6.553434	-0.033865	3.325661
167.739313	3708.389366	6.558438	-0.033916	3.329067
168.090166	3716.442706	6.563443	-0.033987	3.332493
168.135444	3724.510567	6.568448	-0.034001	3.335910
168.414194	3732.471817	6.573453	-0.034058	3.339287
168.994192	3740.487503	6.578458	-0.034172	3.342695
169.134974	3748.548320	6.583462	-0.034203	3.346102
169.202726	3756.598567	6.588467	-0.034221	3.349498
169.505998	3764.634436	6.593472	-0.034283	3.352894
169.822570	3772.665577	6.598477	-0.034348	3.356284
170.158292	3780.652071	6.603482	-0.034416	3.359653
170.481988	3788.657453	6.608486	-0.034481	3.363026
170.675506	3796.707506	6.613491	-0.034523	3.366410
170.830497	3804.746689	6.618496	-0.034557	3.369784
170.952703	3812.793076	6.623501	-0.034586	3.373157
171.384207	3820.850393	6.628506	-0.034671	3.376541
171.579575	3828.839605	6.633510	-0.034713	3.379886
171.737007	3836.869981	6.638515	-0.034748	3.383243
171.860784	3844.912757	6.643520	-0.034777	3.386601
172.019196	3852.940414	6.648525	-0.034812	3.389950
172.188289	3861.052513	6.653530	-0.034849	3.393332
172.428525	3869.063126	6.658534	-0.034899	3.396670
172.878464	3877.018300	6.663539	-0.034988	3.399989
172.990809	3885.029997	6.668544	-0.035015	3.403317
173.159695	3893.047898	6.673549	-0.035051	3.406646
173.476412	3901.063700	6.678554	-0.035116	3.409976
173.697680	3909.081820	6.683558	-0.035163	3.413300
173.895047	3917.136302	6.688563	-0.035205	3.416635
174.132312	3925.142498	6.693568	-0.035255	3.419949
174.414841	3933.150577	6.698573	-0.035313	3.423261
174.897472	3941.200144	6.703578	-0.035408	3.426594
175.189166	3949.205900	6.708582	-0.035468	3.429900
175.544939	3957.275808	6.713587	-0.035540	3.433230
175.581051	3965.331146	6.718592	-0.035552	3.436541
175.688642	3973.297896	6.723597	-0.035577	3.439814
176.093663	3981.316700	6.728602	-0.035658	3.443116
176.325445	3989.351331	6.733606	-0.035707	3.446415
176.390970	3997.416370	6.738611	-0.035724	3.449717
176.500380	4005.469595	6.743616	-0.035750	3.453014
176.731098	4013.478760	6.748621	-0.035799	3.456293
176.927898	4021.496837	6.753626	-0.035841	3.459571
177.120827	4029.512968	6.758630	-0.035882	3.462845
177.458359	4037.565885	6.763635	-0.035951	3.466136
177.750026	4045.575771	6.768640	-0.036010	3.469405
178.032340	4053.634053	6.773645	-0.036069	3.472690
178.398161	4061.681181	6.778650	-0.036142	3.475970
178.441935	4069.624518	6.783654	-0.036156	3.479194
178.599556	4077.687248	6.788659	-0.036191	3.482468
178.774758	4085.704586	6.793664	-0.036229	3.485720
179.092076	4093.679752	6.798669	-0.036293	3.488957
179.319471	4101.751423	6.803674	-0.036341	3.492227
179.352498	4109.808823	6.808678	-0.036353	3.495482
179.473263	4117.802669	6.813683	-0.036381	3.498711
179.706866	4125.837039	6.818688	-0.036430	3.501957
180.032024	4133.821472	6.823693	-0.036496	3.505183
180.123641	4141.879600	6.828698	-0.036518	3.508428
180.081545	4149.936899	6.833702	-0.036516	3.511665
180.291672	4157.972113	6.838707	-0.036561	3.514899
180.550079	4165.974539	6.843712	-0.036614	3.518118
180.778395	4173.966463	6.848717	-0.036662	3.521328
180.900079	4181.970813	6.853722	-0.036690	3.524538
181.040848	4190.009171	6.858726	-0.036722	3.527758
181.466999	4198.046559	6.863731	-0.036807	3.530984
181.845552	4206.067735	6.868736	-0.036883	3.534199
181.957878	4214.125902	6.873741	-0.036909	3.537418
182.226105	4222.148380	6.878746	-0.036965	3.540625
182.426048	4230.144183	6.883750	-0.037007	3.543815
182.550682	4238.203955	6.888755	-0.037036	3.547026
182.707286	4246.231781	6.893760	-0.037071	3.550223
182.750571	4254.363441	6.898765	-0.037084	3.553454
183.055870	4262.374430	6.903770	-0.037147	3.556642
183.092443	4270.309490	6.908774	-0.037159	3.559789
183.398578	4278.309710	6.913779	-0.037221	3.562967
183.579042	4286.328072	6.918784	-0.037260	3.566146
183.623642	4294.331292	6.923789	-0.037274	3.569312
183.911015	4302.418697	6.928794	-0.037333	3.572516
184.174313	4310.408437	6.933798	-0.037388	3.575677
184.303716	4318.427030	6.938803	-0.037417	3.578843
184.595711	4326.451257	6.943808	-0.037477	3.582013
184.864210	4334.418584	6.948813	-0.037533	3.585157
184.849874	4342.504844	6.953818	-0.037536	3.588337
184.945399	4350.550601	6.958822	-0.037559	3.591502
185.268133	4358.557703	6.963827	-0.037624	3.594655
185.803002	4366.544009	6.968832	-0.037729	3.597803
185.824256	4374.574358	6.973837	-0.037739	3.600951
186.103590	4382.593311	6.978842	-0.037796	3.604099
186.280822	4390.610717	6.983846	-0.037835	3.607240
186.349459	4398.654904	6.988851	-0.037853	3.610387
186.417709	4406.746160	6.993856	-0.037871	3.613549
186.634852	4414.715555	6.998861	-0.037917	3.616664
186.884207	4422.736923	7.003866	-0.037969	3.619799
186.951457	4430.739675	7.008870	-0.037987	3.622918
187.002672	4438.791414	7.013875	-0.038002	3.626053
187.192473	4446.862956	7.018880	-0.038043	3.629197
187.217281	4454.862248	7.023885	-0.038053	3.632305
187.601842	4462.929500	7.028890	-0.038130	3.635447
187.693195	4470.905853	7.033894	-0.038153	3.638543
188.141144	4478.905508	7.038899	-0.038242	3.641655
188.171491	4486.931316	7.043904	-0.038253	3.644764
188.360131	4494.907904	7.048909	-0.038293	3.647854
188.536961	4502.991551	7.053914	-0.038332	3.650984
188.679167	4511.015841	7.058918	-0.038364	3.654086
188.856831	4519.051891	7.063923	-0.038402	3.657192
189.141368	4527.055191	7.068928	-0.038461	3.660285
189.234105	4535.051633	7.073933	-0.038484	3.663367
189.596565	4543.112109	7.078938	-0.038557	3.666479
189.790747	4551.133270	7.083942	-0.038598	3.669569
189.951159	4559.184690	7.088947	-0.038634	3.672666
190.255976	4567.228435	7.093952	-0.038696	3.675762
190.383305	4575.165556	7.098957	-0.038725	3.678810
190.630536	4583.232549	7.103962	-0.038777	3.681908
190.699287	4591.199217	7.108966	-0.038795	3.684960
190.994587	4599.248962	7.113971	-0.038855	3.688047
191.333982	4607.319840	7.118976	-0.038924	3.691141
191.519985	4615.289990	7.123981	-0.038964	3.694190
191.684284	4623.364810	7.128986	-0.039000	3.697276
191.694438	4631.325487	7.133990	-0.039008	3.700312
191.927569	4639.333913	7.138995	-0.039056	3.703369
192.322526	4647.417309	7.144000	-0.039135	3.706456
192.305024	4655.393952	7.149005	-0.039138	3.709490
192.905206	4663.485128	7.154010	-0.039255	3.712579
193.019745	4671.573488	7.159014	-0.039282	3.715654
193.271073	4679.521523	7.164019	-0.039334	3.718675
193.763820	4687.517525	7.169024	-0.039431	3.721719
193.924886	4695.460671	7.174029	-0.039467	3.724732
194.131311	4703.535347	7.179034	-0.039511	3.727793
194.151688	4711.588097	7.184038	-0.039520	3.730838
194.432938	4719.606142	7.189043	-0.039578	3.733875
194.694699	4727.627112	7.194048	-0.039632	3.736910
194.805169	4735.624498	7.199053	-0.039658	3.739929
194.974244	4743.674445	7.204058	-0.039695	3.742967
195.225843	4751.671956	7.209062	-0.039747	3.745986
195.520519	4759.686630	7.214067	-0.039808	3.749009
195.719826	4767.762840	7.219072	-0.039850	3.752050
196.102899	4775.731242	7.224077	-0.039927	3.755053
196.071289	4783.779209	7.229082	-0.039927	3.758073
196.238949	4791.818057	7.234086	-0.039963	3.761093
196.723651	4799.799839	7.239091	-0.040059	3.764095
196.941299	4807.852910	7.244096	-0.040105	3.767116
196.977109	4815.845169	7.249101	-0.040117	3.770108
197.253485	4823.926922	7.254106	-0.040174	3.773136
197.509838	4831.966349	7.259110	-0.040228	3.776145
197.587851	4839.947770	7.264115	-0.040248	3.779126
197.930126	4847.985789	7.269120	-0.040317	3.782132
198.042685	4855.966198	7.274125	-0.040343	3.785109
198.281042	4863.989878	7.279130	-0.040393	3.788102
198.433102	4872.062088	7.284134	-0.040427	3.791109
198.786934	4880.080082	7.289139	-0.040498	3.794098
198.831020	4888.110279	7.294144	-0.040512	3.797083
198.827325	4896.075601	7.299149	-0.040517	3.800040
199.291454	4904.089517	7.304154	-0.040609	3.803022
199.282724	4912.119944	7.309158	-0.040612	3.805999
199.448986	4920.112709	7.314163	-0.040649	3.808962
199.946961	4928.168432	7.319168	-0.040747	3.811954
200.120126	4936.209851	7.324173	-0.040785	3.814931
200.217793	4944.227341	7.329178	-0.040809	3.817896
200.449653	4952.243380	7.334182	-0.040857	3.820860
200.719381	4960.218706	7.339187	-0.040913	3.823808
200.914553	4968.282530	7.344192	-0.040955	3.826784
200.919200	4976.282185	7.349197	-0.040961	3.829731
201.287893	4984.373398	7.354202	-0.041035	3.832716
201.326510	4992.360692	7.359206	-0.041048	3.835654
201.403207	5000.358785	7.364211	-0.041068	3.838595
201.577792	5008.391569	7.369216	-0.041106	3.841548
201.859956	5016.324139	7.374221	-0.041164	3.844464
201.921703	5024.439592	7.379226	-0.041181	3.847441
201.933331	5032.450763	7.384230	-0.041188	3.850376
202.474869	5040.477911	7.389235	-0.041295	3.853325
202.633142	5048.530076	7.394240	-0.041330	3.856274
202.473387	5056.501745	7.399245	-0.041305	3.859184
202.881834	5064.582446	7.404250	-0.041387	3.862143
203.059569	5072.530663	7.409254	-0.041425	3.865047
203.055197	5080.607067	7.414259	-0.041430	3.867992
203.309440	5088.665302	7.419264	-0.041483	3.870934
203.449547	5096.915244	7.424269	-0.041515	3.873940
203.717085	5104.865185	7.429274	-0.041570	3.876838
203.901830	5112.779251	7.434278	-0.041610	3.879718
204.049368	5120.739965	7.439283	-0.041643	3.882613
204.368208	5128.718204	7.444288	-0.041708	3.885515
204.641368	5136.708425	7.449293	-0.041764	3.888419
204.749347	5144.773807	7.454298	-0.041789	3.891344
204.996410	5152.772436	7.459302	-0.041841	3.894246
205.057592	5160.802448	7.464307	-0.041858	3.897153
205.212091	5168.832740	7.469312	-0.041892	3.900060
205.388351	5176.805732	7.474317	-0.041930	3.902944
205.478679	5184.839338	7.479322	-0.041953	3.905847
205.473530	5192.883044	7.484326	-0.041957	3.908749
205.588614	5200.917003	7.489331	-0.041984	3.911648
205.890121	5208.959537	7.494336	-0.042046	3.914551
205.707780	5216.947061	7.499341	-0.042017	3.917423
205.920813	5224.945391	7.504346	-0.042062	3.920304
206.186869	5232.966992	7.509350	-0.042117	3.923193
206.347318	5240.973888	7.514355	-0.042153	3.926072
206.467814	5249.003543	7.519360	-0.042181	3.928956
206.922839	5257.039774	7.524365	-0.042271	3.931847
207.063577	5265.094357	7.529370	-0.042303	3.934736
207.117912	5273.089471	7.534374	-0.042318	3.937601
207.263496	5281.054494	7.539379	-0.042351	3.940454
207.420668	5289.092029	7.544384	-0.042386	3.943331
207.286876	5297.123620	7.549389	-0.042366	3.946199
207.504838	5305.150747	7.554394	-0.042412	3.949070
207.743017	5313.180202	7.559398	-0.042462	3.951939
207.919571	5321.211594	7.564403	-0.042500	3.954806
208.100676	5329.230269	7.569408	-0.042540	3.957666
208.384943	5337.168277	7.574413	-0.042598	3.960498
208.668640	5345.194630	7.579418	-0.042656	3.963358
208.787713	5353.233915	7.584422	-0.042684	3.966219
209.045506	5361.228494	7.589427	-0.042737	3.969064
209.356686	5369.299405	7.594432	-0.042801	3.971934
209.378882	5377.330100	7.599437	-0.042811	3.974784
209.929078	5385.361087	7.604442	-0.042918	3.977640
209.983086	5393.374637	7.609446	-0.042934	3.980480
210.094080	5401.371869	7.614451	-0.042960	3.983313
210.159472	5409.441419	7.619456	-0.042978	3.986168
210.347736	5417.428052	7.624461	-0.043018	3.988995
210.687666	5425.473560	7.629466	-0.043087	3.991842
210.788108	5433.491727	7.634470	-0.043111	3.994674
210.949599	5441.522582	7.639475	-0.043147	3.997510
211.339450	5449.519575	7.644480	-0.043225	4.000335
211.150043	5457.527382	7.649485	-0.043195	4.003152
211.524793	5465.572071	7.654490	-0.043270	4.005990
211.787155	5473.563753	7.659494	-0.043325	4.008805
211.786546	5481.612926	7.664499	-0.043330	4.011634
211.809434	5489.670299	7.669504	-0.043340	4.014465
211.948336	5497.673060	7.674509	-0.043371	4.017276
212.377196	5505.662449	7.679514	-0.043457	4.020085
212.633565	5513.682131	7.684518	-0.043510	4.022899
212.637172	5521.694538	7.689523	-0.043516	4.025706
212.972801	5529.733764	7.694528	-0.043584	4.028525
213.209584	5537.742877	7.699533	-0.043634	4.031329
213.284758	5545.884396	7.704538	-0.043653	4.034176
213.570796	5553.870622	7.709542	-0.043712	4.036970
213.812192	5561.789252	7.714547	-0.043762	4.039737
213.824198	5569.827068	7.719552	-0.043770	4.042541
214.186671	5577.786611	7.724557	-0.043843	4.045320
214.529657	5585.819863	7.729562	-0.043912	4.048123
214.383783	5593.890151	7.734566	-0.043891	4.050930
214.370931	5601.919111	7.739571	-0.043894	4.053722
214.673082	5609.964754	7.744576	-0.043955	4.056523
214.745197	5617.879957	7.749581	-0.043974	4.059273
214.907985	5625.937193	7.754586	-0.044010	4.062072
215.286094	5633.905681	7.759590	-0.044086	4.064841
215.473002	5641.957864	7.764595	-0.044126	4.067635
215.623327	5649.960350	7.769600	-0.044160	4.070408
215.769140	5657.994715	7.774605	-0.044192	4.073191
215.995654	5666.071122	7.779610	-0.044240	4.075988
216.109181	5674.048379	7.784614	-0.044267	4.078747
216.418513	5682.055830	7.789619	-0.044330	4.081517
216.643724	5690.040531	7.794624	-0.044377	4.084276
216.819140	5698.075252	7.799629	-0.044415	4.087050
216.927119	5706.148063	7.804634	-0.044441	4.089834
217.078245	5714.191195	7.809638	-0.044475	4.092607
217.211068	5722.164355	7.814643	-0.044505	4.095354
217.524376	5730.181335	7.819648	-0.044569	4.098116
217.757131	5738.196063	7.824653	-0.044617	4.100874
217.876770	5746.223355	7.829658	-0.044645	4.103633
218.016472	5754.229870	7.834662	-0.044677	4.106384
217.959503	5762.251102	7.839667	-0.044671	4.109135
218.348657	5770.297291	7.844672	-0.044749	4.111898
218.452874	5778.329681	7.849677	-0.044774	4.114652
218.621687	5786.349583	7.854682	-0.044811	4.117400
219.123442	5794.313257	7.859686	-0.044910	4.120131
219.351973	5802.337287	7.864691	-0.044958	4.122877
219.421807	5810.357982	7.869696	-0.044977	4.125619
219.422291	5818.379268	7.874701	-0.044982	4.128357
219.645561	5826.431648	7.879706	-0.045029	4.131108
219.678295	5834.467998	7.884710	-0.045041	4.133849
219.732048	5842.472288	7.889715	-0.045056	4.136577
219.941413	5850.485493	7.894720	-0.045101	4.139309
220.239546	5858.526619	7.899725	-0.045162	4.142049
220.420746	5866.502960	7.904730	-0.045201	4.144764
220.548643	5874.573786	7.909734	-0.045230	4.147508
220.797422	5882.553835	7.914739	-0.045282	4.150222
221.078042	5890.620918	7.919744	-0.045340	4.152963
221.278703	5898.605993	7.924749	-0.045383	4.155674
221.544001	5906.596910	7.929754	-0.045438	4.158386
221.651260	5914.665874	7.934758	-0.045463	4.161120
221.571646	5922.637699	7.939763	-0.045454	4.163818
221.904837	5930.677317	7.944768	-0.045521	4.166541
222.084068	5938.692419	7.949773	-0.045560	4.169253
222.281782	5946.726069	7.954778	-0.045602	4.171970
222.459429	5954.729637	7.959782	-0.045641	4.174674
222.814648	5962.763147	7.964787	-0.045713	4.177389
222.811635	5970.773063	7.969792	-0.045718	4.180089
222.756966	5978.743514	7.974797	-0.045713	4.182775
222.903600	5986.790433	7.979802	-0.045746	4.185486
223.125124	5994.825372	7.984806	-0.045792	4.188193
223.203707	6002.823765	7.989811	-0.045812	4.190883
223.561787	6010.975458	7.994816	-0.045885	4.193627
223.609641	6018.958378	7.999821	-0.045899	4.196309
223.606495	6026.894077	8.004826	-0.045904	4.198973
223.876677	6034.911912	8.009830	-0.045960	4.201665
224.284363	6042.872969	8.014835	-0.046041	4.204338
224.340357	6050.962942	8.019840	-0.046057	4.207049
224.280037	6058.893834	8.024845	-0.046051	4.209703
224.482835	6066.964488	8.029850	-0.046095	4.212406
224.727595	6074.977499	8.034854	-0.046146	4.215088
224.796236	6082.979536	8.039859	-0.046164	4.217762
225.002788	6091.025575	8.044864	-0.046208	4.220451
225.127732	6099.019376	8.049869	-0.046237	4.223120
225.258933	6107.021854	8.054874	-0.046266	4.225791
225.417895	6115.086733	8.059878	-0.046302	4.228480
225.590615	6123.083286	8.064883	-0.046339	4.231145
225.668188	6131.108357	8.069888	-0.046359	4.233818
225.641070	6139.149063	8.074893	-0.046360	4.236492
225.932532	6147.104950	8.079898	-0.046419	4.239140
226.111183	6155.173478	8.084902	-0.046458	4.241822
226.215076	6163.133614	8.089907	-0.046483	4.244466
226.575613	6171.242160	8.094912	-0.046555	4.247160
226.735773	6179.196775	8.099917	-0.046591	4.249800
226.769793	6187.262608	8.104922	-0.046603	4.252473
227.004645	6195.277111	8.109926	-0.046652	4.255130
227.288370	6203.287847	8.114931	-0.046710	4.257784
227.454792	6211.294603	8.119936	-0.046747	4.260434
227.425408	6219.323956	8.124941	-0.046747	4.263088
227.655238	6227.328714	8.129946	-0.046795	4.265734
227.964097	6235.359156	8.134950	-0.046858	4.268388
227.904613	6243.373167	8.139955	-0.046852	4.271032
228.334733	6251.466499	8.144960	-0.046938	4.273704
228.485074	6259.427321	8.149965	-0.046971	4.276329
228.574349	6267.402256	8.154970	-0.046993	4.278956
228.711498	6275.449235	8.159974	-0.047024	4.281606
228.996636	6283.393080	8.164979	-0.047083	4.284221
229.345899	6291.481850	8.169984	-0.047154	4.286883
229.287703	6299.479469	8.174989	-0.047148	4.289510
229.762158	6307.570601	8.179994	-0.047242	4.292170
230.050155	6315.565870	8.184998	-0.047301	4.294796
229.956521	6323.576385	8.190003	-0.047289	4.297421
230.246265	6331.573948	8.195008	-0.047349	4.300045
230.398676	6339.609365	8.200013	-0.047382	4.302677
230.540845	6347.599445	8.205018	-0.047414	4.305294
230.583429	6355.635939	8.210022	-0.047428	4.307923
230.846194	6363.639749	8.215027	-0.047482	4.310541
231.124683	6371.701707	8.220032	-0.047540	4.313177
231.187939	6379.715309	8.225037	-0.047557	4.315794
231.285931	6387.677506	8.230042	-0.047581	4.318393
231.453165	6395.662138	8.235046	-0.047617	4.320998
231.725632	6403.678058	8.240051	-0.047673	4.323612
231.969925	6411.719708	8.245056	-0.047724	4.326233
232.032481	6419.708931	8.250061	-0.047741	4.328834
232.420378	6427.807270	8.255066	-0.047819	4.331471
232.540054	6435.824279	8.260070	-0.047847	4.334078
232.678083	6443.791952	8.265075	-0.047878	4.336668
233.015551	6451.837166	8.270080	-0.047947	4.339283
233.121867	6459.853736	8.275085	-0.047972	4.341885
233.320681	6467.812577	8.280090	-0.048014	4.344467
233.563850	6475.868788	8.285094	-0.048065	4.347080
233.597206	6483.861927	8.290099	-0.048077	4.349669
233.840578	6491.964614	8.295104	-0.048128	4.352294
234.060002	6500.015827	8.300109	-0.048174	4.354900
234.339775	6507.995427	8.305114	-0.048231	4.357482
234.167036	6515.956871	8.310118	-0.048205	4.360054
234.327261	6523.915514	8.315123	-0.048240	4.362625
234.652042	6531.962841	8.320128	-0.048306	4.365224
234.800291	6539.974898	8.325133	-0.048339	4.367810
234.886565	6547.998750	8.330138	-0.048361	4.370397
235.208498	6556.088916	8.335142	-0.048426	4.373005
235.258345	6564.086265	8.340147	-0.048441	4.375581
235.339445	6572.083900	8.345152	-0.048461	4.378155
235.457013	6580.059405	8.350157	-0.048489	4.380721
235.815606	6588.042132	8.355162	-0.048561	4.383288
236.013910	6596.109330	8.360166	-0.048603	4.385881
235.870117	6604.093986	8.365171	-0.048582	4.388443
236.270183	6612.166321	8.370176	-0.048662	4.391036
236.292071	6620.187730	8.375181	-0.048672	4.393608
236.312280	6628.224605	8.380186	-0.048681	4.396184
236.666842	6636.191392	8.385190	-0.048752	4.398737
236.726003	6644.214667	8.390195	-0.048769	4.401305
237.045607	6652.221814	8.395200	-0.048834	4.403869
237.312421	6660.273685	8.400205	-0.048889	4.406444
237.651381	6668.207061	8.405210	-0.048958	4.408981
237.709706	6676.311903	8.410214	-0.048974	4.411569
237.786460	6684.316548	8.415219	-0.048994	4.414124
238.162376	6692.394712	8.420224	-0.049069	4.416703
238.220758	6700.341493	8.425229	-0.049086	4.419236
238.442167	6708.394332	8.430234	-0.049132	4.421803
238.713462	6716.393342	8.435238	-0.049188	4.424351
238.773957	6724.409963	8.440243	-0.049205	4.426902
238.962285	6732.438243	8.445248	-0.049246	4.429457
238.987661	6740.473548	8.450253	-0.049256	4.432011
239.189570	6748.528735	8.455258	-0.049299	4.434570
239.244145	6756.514954	8.460262	-0.049315	4.437106
239.380877	6764.426901	8.465267	-0.049346	4.439617
239.723779	6772.528721	8.470272	-0.049415	4.442188
239.902902	6780.470030	8.475277	-0.049454	4.444705
239.942904	6788.533082	8.480282	-0.049467	4.447259
240.159199	6796.564995	8.485286	-0.049512	4.449803
240.337665	6804.566540	8.490291	-0.049551	4.452335
240.533403	6812.625837	8.495296	-0.049593	4.454884
240.534556	6820.650711	8.500301	-0.049599	4.457420
240.861786	6828.611970	8.505306	-0.049665	4.459936
241.116636	6836.691503	8.510310	-0.049718	4.462487
241.183000	6844.625518	8.515315	-0.049736	4.464991
241.348979	6852.691639	8.520320	-0.049772	4.467534
241.459829	6860.677823	8.525325	-0.049798	4.470051
241.622959	6868.734419	8.530330	-0.049834	4.472589
241.628286	6876.741817	8.535334	-0.049841	4.475110
241.653369	6884.748565	8.540339	-0.049851	4.477628
241.910829	6892.718668	8.545344	-0.049904	4.480135
241.853159	6900.783048	8.550349	-0.049899	4.482669
242.280601	6908.720794	8.555354	-0.049984	4.485163
242.444275	6916.802054	8.560359	-0.050020	4.487700
242.469588	6924.787757	8.565363	-0.050030	4.490205
242.790714	6932.853820	8.570368	-0.050096	4.492735
242.928290	6940.876438	8.575373	-0.050127	4.495249
243.122369	6948.893124	8.580378	-0.050168	4.497760
243.364208	6956.909957	8.585383	-0.050219	4.500270
243.392835	6964.847370	8.590387	-0.050230	4.502753
243.715150	6972.895560	8.595392	-0.050295	4.505270
243.761185	6980.896716	8.600397	-0.050309	4.507770
243.901994	6988.938571	8.605402	-0.050341	4.510281
244.176714	6997.006923	8.610407	-0.050398	4.512800
244.181858	7005.021918	8.615411	-0.050404	4.515300
244.280084	7013.036656	8.620416	-0.050428	4.517799
244.547546	7020.978460	8.625421	-0.050483	4.520274
244.597995	7028.983445	8.630426	-0.050498	4.522767
244.644404	7037.004943	8.635431	-0.050512	4.525264
244.770627	7044.970121	8.640435	-0.050541	4.527742
244.953243	7053.050848	8.645440	-0.050580	4.530254
244.958648	7061.080990	8.650445	-0.050587	4.532750
245.162678	7069.069084	8.655450	-0.050630	4.535231
245.484122	7077.119295	8.660455	-0.050696	4.537730
245.430373	7085.103771	8.665459	-0.050691	4.540206
245.740858	7093.171134	8.670464	-0.050755	4.542708
245.733292	7101.141995	8.675469	-0.050759	4.545178
245.996810	7109.170236	8.680474	-0.050813	4.547665
246.230858	7117.212212	8.685479	-0.050862	4.550154
246.466713	7125.239503	8.690483	-0.050912	4.552638
246.577848	7133.241554	8.695488	-0.050938	4.555112
246.504479	7141.247815	8.700493	-0.050930	4.557586
246.893621	7149.230153	8.705498	-0.051008	4.560052
247.247882	7157.320310	8.710503	-0.051079	4.562549
247.277461	7165.240160	8.715507	-0.051090	4.564992
247.292367	7173.310173	8.720512	-0.051098	4.567481
247.454817	7181.314167	8.725517	-0.051134	4.569947
247.630870	7189.391461	8.730522	-0.051172	4.572435
247.909573	7197.399873	8.735527	-0.051230	4.574901
248.068053	7205.407992	8.740531	-0.051265	4.577365
248.276060	7213.405130	8.745536	-0.051309	4.579824
248.473329	7221.446312	8.750541	-0.051351	4.582295
248.770270	7229.401205	8.755546	-0.051412	4.584739
249.035192	7237.507019	8.760551	-0.051467	4.587227
249.077636	7245.448812	8.765555	-0.051480	4.589664
249.143685	7253.525160	8.770560	-0.051498	4.592141
249.266706	7261.529398	8.775565	-0.051526	4.594594
249.589969	7269.598874	8.780570	-0.051592	4.597066
249.615035	7277.513021	8.785575	-0.051602	4.599489
249.629445	7285.537506	8.790579	-0.051610	4.601944
249.932148	7293.530340	8.795584	-0.051672	4.604389
249.955910	7301.600236	8.800589	-0.051682	4.606856
250.073796	7309.522135	8.805594	-0.051709	4.609276
250.531523	7317.609793	8.810599	-0.051800	4.611745
250.410195	7325.628270	8.815603	-0.051783	4.614192
250.419579	7333.681711	8.820608	-0.051790	4.616649
250.701555	7341.638157	8.825613	-0.051848	4.619074
250.955619	7349.672681	8.830618	-0.051901	4.621522
251.001233	7357.629361	8.835623	-0.051915	4.623945
251.096401	7365.702128	8.840627	-0.051938	4.626402
251.317462	7373.697259	8.845632	-0.051985	4.628834
251.466542	7381.726373	8.850637	-0.052018	4.631275
251.683446	7389.764010	8.855642	-0.052064	4.633718
252.112240	7397.809447	8.860647	-0.052149	4.636161
252.131346	7405.764868	8.865651	-0.052158	4.638576
252.158711	7413.823281	8.870656	-0.052169	4.641021
252.326633	7421.753447	8.875661	-0.052206	4.643425
252.437837	7429.803054	8.880666	-0.052232	4.645865
252.754431	7437.809059	8.885671	-0.052296	4.648290
252.816525	7445.840281	8.890675	-0.052313	4.650721
253.049013	7453.886598	8.895680	-0.052362	4.653156
253.029543	7461.905405	8.900685	-0.052364	4.655581
253.143579	7469.849319	8.905690	-0.052391	4.657982
253.534647	7477.940031	8.910695	-0.052469	4.660426
253.703985	7485.899831	8.915699	-0.052506	4.662829
253.795402	7493.921434	8.920704	-0.052528	4.665250
253.860887	7501.971982	8.925709	-0.052546	4.667678
254.104399	7509.967484	8.930714	-0.052597	4.670088
254.156642	7518.125915	8.935719	-0.052612	4.672547
254.260287	7526.127168	8.940723	-0.052637	4.674956
254.730041	7534.109570	8.945728	-0.052730	4.677358
254.642875	7542.008194	8.950733	-0.052719	4.679735
254.891313	7549.988466	8.955738	-0.052771	4.682134
255.012800	7558.049101	8.960743	-0.052799	4.684556
255.154243	7566.074577	8.965747	-0.052831	4.686967
255.187577	7574.044302	8.970752	-0.052842	4.689360
255.303585	7582.106054	8.975757	-0.052870	4.691778
255.367638	7590.116500	8.980762	-0.052887	4.694181
255.530442	7598.169243	8.985767	-0.052923	4.696594
255.629624	7606.075675	8.990771	-0.052947	4.698963
255.979981	7614.211078	8.995776	-0.053017	4.701399
255.967149	7622.152057	9.000781	-0.053020	4.703775
256.120171	7630.140046	9.005786	-0.053054	4.706165
256.374737	7638.225892	9.010791	-0.053107	4.708582
256.552847	7646.231803	9.015795	-0.053146	4.710974
256.726228	7654.256460	9.020800	-0.053184	4.713370
256.823447	7662.297201	9.025805	-0.053207	4.715770
256.847655	7670.254604	9.030810	-0.053217	4.718145
257.114436	7678.293515	9.035815	-0.053272	4.720542
256.910474	7686.283235	9.040819	-0.053240	4.722924
257.314136	7694.308595	9.045824	-0.053321	4.725313
257.528464	7702.363707	9.050829	-0.053366	4.727711
257.439093	7710.383422	9.055834	-0.053355	4.730099
257.640808	7718.434099	9.060839	-0.053398	4.732493
257.787044	7726.407522	9.065843	-0.053431	4.734863
257.853708	7734.443057	9.070848	-0.053449	4.737251
257.980737	7742.394980	9.075853	-0.053478	4.739612
258.144954	7750.440723	9.080858	-0.053514	4.742000
258.392459	7758.417801	9.085863	-0.053565	4.744366
258.329971	7766.444068	9.090867	-0.053559	4.746747
258.657815	7774.507068	9.095872	-0.053626	4.749136
259.058369	7782.522371	9.100877	-0.053706	4.751509
259.098953	7790.606308	9.105882	-0.053719	4.753903
259.230999	7798.599384	9.110887	-0.053749	4.756268
259.433892	7806.545602	9.115891	-0.053792	4.758618
259.476365	7814.561515	9.120896	-0.053805	4.760988
259.559352	7822.536500	9.125901	-0.053826	4.763344
259.830030	7830.562189	9.130906	-0.053882	4.765714
260.141243	7838.571337	9.135911	-0.053946	4.768077
260.084669	7846.629652	9.140915	-0.053941	4.770455
260.218225	7854.647841	9.145920	-0.053971	4.772820
260.549526	7862.681130	9.150925	-0.054038	4.775187
260.614827	7870.656709	9.155930	-0.054056	4.777536
260.909202	7878.656305	9.160935	-0.054116	4.779891
260.915518	7886.687853	9.165939	-0.054123	4.782255
261.159727	7894.678921	9.170944	-0.054174	4.784605
261.166166	7902.742889	9.175949	-0.054180	4.786976
261.516289	7910.675517	9.180954	-0.054251	4.789306
261.565652	7918.795960	9.185959	-0.054266	4.791691
261.481645	7926.772811	9.190963	-0.054256	4.794033
261.940262	7934.800970	9.195968	-0.054346	4.796387
262.188887	7942.780060	9.200973	-0.054398	4.798727
262.074207	7950.800214	9.205978	-0.054382	4.801079
262.329440	7958.792678	9.210983	-0.054435	4.803419
262.355912	7966.844212	9.215987	-0.054446	4.805777
262.772744	7974.864294	9.220992	-0.054529	4.808123
262.637695	7982.858273	9.225997	-0.054509	4.810463
262.957489	7990.324253	9.231002	-0.054574	4.812645
263.007097	7995.066595	9.236007	-0.054586	4.814031

263.028549	7997.635863	9.241011	-0.054592	4.814782
263.230590	7999.058942	9.246016	-0.054631	4.815197
263.497262	7999.486409	9.251021	-0.054681	4.815321
263.423602	8000.449980	9.256026	-0.054669	4.815602
263.476848	8000.514985	9.261031	-0.054679	4.815621
263.504626	8000.490891	9.266035	-0.054684	4.815614
263.688647	8000.483257	9.271040	-0.054719	4.815611
263.725635	8000.462520	9.276045	-0.054726	4.815605
263.873309	8000.457494	9.281050	-0.054754	4.815602
263.961131	8000.539095	9.286055	-0.054770	4.815626
264.114575	8000.449757	9.291059	-0.054799	4.815599
264.099956	8000.517919	9.296064	-0.054797	4.815619
264.163145	8000.504024	9.301069	-0.054809	4.815615
264.220006	8000.471860	9.306074	-0.054819	4.815605
264.209372	8000.576416	9.311079	-0.054818	4.815636
264.153605	8000.447308	9.316083	-0.054808	4.815598
264.413525	8000.521057	9.321088	-0.054856	4.815618
264.296465	8000.538386	9.326093	-0.054835	4.815624
264.268066	8000.464218	9.331098	-0.054830	4.815602
264.667248	8000.472948	9.336103	-0.054904	4.815603
264.639531	8000.503500	9.341107	-0.054899	4.815612
264.762662	8000.504481	9.346112	-0.054923	4.815612
264.744794	8000.505278	9.351117	-0.054920	4.815612
264.715161	8000.462075	9.356122	-0.054914	4.815600
264.719190	8000.516655	9.361127	-0.054915	4.815616
264.822572	8000.523722	9.366131	-0.054935	4.815617
264.852420	8000.424870	9.371136	-0.054941	4.815588
264.723785	8000.523210	9.376141	-0.054917	4.815617
264.729319	8000.462422	9.381146	-0.054918	4.815600
264.913964	8000.575536	9.386151	-0.054953	4.815632
264.885868	8000.429785	9.391155	-0.054948	4.815589
265.016353	8000.545214	9.396160	-0.054972	4.815622
264.915554	8000.549988	9.401165	-0.054954	4.815624
265.051211	8000.422960	9.406170	-0.054979	4.815587
265.102728	8000.570211	9.411175	-0.054989	4.815629
265.031583	8000.500680	9.416179	-0.054976	4.815609
265.278229	8000.527202	9.421184	-0.055022	4.815616
265.282759	8000.461054	9.426189	-0.055024	4.815596
265.204871	8000.551683	9.431194	-0.055009	4.815623
265.215973	8000.479232	9.436199	-0.055012	4.815602
265.153934	8000.457933	9.441203	-0.055000	4.815596
265.182820	8000.454157	9.446208	-0.055006	4.815595
265.339394	8000.571085	9.451213	-0.055035	4.815628
265.205235	8000.511201	9.456218	-0.055011	4.815611
265.280848	8000.487894	9.461223	-0.055025	4.815604
265.304383	8000.546002	9.466227	-0.055030	4.815621
265.437589	8000.438165	9.471232	-0.055055	4.815589
265.376912	8000.596392	9.476237	-0.055044	4.815636
265.242614	8000.433932	9.481242	-0.055019	4.815589
265.743684	8000.591794	9.486247	-0.055113	4.815632
265.687553	8000.476564	9.491251	-0.055102	4.815599
265.634223	8000.497078	9.496256	-0.055093	4.815605
265.760333	8000.582520	9.501261	-0.055116	4.815630
265.783845	8000.497451	9.506266	-0.055121	4.815605
265.763781	8000.452267	9.511271	-0.055117	4.815592
265.662255	8000.507248	9.516275	-0.055099	4.815608
265.909507	8000.555151	9.521280	-0.055145	4.815621
265.963366	8000.519732	9.526285	-0.055155	4.815610
265.965958	8000.453551	9.531290	-0.055156	4.815591
266.006723	8000.566437	9.536295	-0.055164	4.815624
265.789326	8000.485948	9.541299	-0.055124	4.815601
265.766641	8000.425762	9.546304	-0.055120	4.815584
265.808080	8000.480960	9.551309	-0.055128	4.815600
265.951188	8000.560271	9.556314	-0.055155	4.815622
266.033243	8000.568057	9.561319	-0.055170	4.815624
265.989384	8000.487220	9.566323	-0.055162	4.815601
266.189889	8000.574957	9.571328	-0.055200	4.815625
266.167628	8000.483790	9.576333	-0.055196	4.815599
266.089164	8000.559453	9.581338	-0.055182	4.815621
266.213829	8000.496351	9.586343	-0.055205	4.815602
266.145596	8000.567907	9.591347	-0.055193	4.815623
266.109088	8000.460479	9.596352	-0.055186	4.815592
266.061101	8000.578315	9.601357	-0.055178	4.815627
266.176418	8000.484072	9.606362	-0.055199	4.815599
266.275172	8000.608600	9.611367	-0.055218	4.815635
266.199630	8000.575323	9.616371	-0.055204	4.815625
266.115757	8000.452155	9.621376	-0.055189	4.815590
266.071869	8000.499537	9.626381	-0.055181	4.815604
265.923646	8000.602900	9.631386	-0.055154	4.815635
266.116337	8000.453302	9.636391	-0.055190	4.815590
266.129400	8000.576417	9.641395	-0.055192	4.815626
266.198925	8000.436543	9.646400	-0.055205	4.815585
266.072098	8000.549875	9.651405	-0.055182	4.815618
266.150994	8000.509526	9.656410	-0.055197	4.815606
266.263620	8000.502856	9.661415	-0.055218	4.815604
266.209911	8000.593885	9.666419	-0.055209	4.815631
266.185723	8000.432166	9.671424	-0.055204	4.815583
266.248410	8000.553962	9.676429	-0.055216	4.815619
266.219488	8000.502220	9.681434	-0.055211	4.815604
266.323465	8000.474038	9.686439	-0.055231	4.815595
266.196185	8000.619417	9.691443	-0.055207	4.815638
266.278146	8000.451967	9.696448	-0.055223	4.815589
266.384362	8000.600125	9.701453	-0.055243	4.815631
266.418150	8000.453250	9.706458	-0.055249	4.815588
266.393221	8000.577877	9.711463	-0.055245	4.815625
266.189191	8000.547826	9.716467	-0.055207	4.815617
266.387196	8000.548974	9.721472	-0.055244	4.815616
266.536064	8000.509778	9.726477	-0.055272	4.815604
266.358287	8000.591284	9.731482	-0.055240	4.815629
266.557318	8000.449269	9.736487	-0.055277	4.815587
266.577200	8000.615238	9.741491	-0.055281	4.815635
266.363006	8000.480306	9.746496	-0.055241	4.815596
266.453650	8000.623933	9.751501	-0.055258	4.815638
266.540775	8000.440540	9.756506	-0.055275	4.815584
266.476999	8000.563459	9.761511	-0.055263	4.815620
266.575887	8000.492452	9.766515	-0.055282	4.815599
266.527134	8000.567536	9.771520	-0.055273	4.815621
266.840734	8000.454121	9.776525	-0.055332	4.815587
266.625608	8000.540354	9.781530	-0.055292	4.815613
266.691331	8000.476281	9.786535	-0.055304	4.815594
266.715487	8000.514099	9.791539	-0.055309	4.815605
266.606791	8000.492030	9.796544	-0.055289	4.815599
266.584623	8000.501304	9.801549	-0.055285	4.815601
266.435682	8000.592902	9.806554	-0.055258	4.815629
266.545932	8000.441944	9.811559	-0.055279	4.815584
266.423023	8000.580985	9.816563	-0.055256	4.815626
266.475737	8000.491053	9.821568	-0.055266	4.815599
266.786905	8000.608397	9.826573	-0.055324	4.815632
266.634363	8000.471274	9.831578	-0.055296	4.815592
266.609924	8000.523251	9.836583	-0.055292	4.815608
266.853976	8000.497376	9.841587	-0.055338	4.815599
266.771578	8000.491767	9.846592	-0.055322	4.815598
266.624425	8000.521421	9.851597	-0.055295	4.815607
266.508020	8000.441525	9.856602	-0.055274	4.815584
266.866870	8000.491269	9.861607	-0.055341	4.815597
266.765514	8000.558007	9.866611	-0.055322	4.815617
266.717246	8000.546549	9.871616	-0.055314	4.815614
266.805214	8000.556570	9.876621	-0.055330	4.815616
266.816260	8000.462745	9.881626	-0.055333	4.815589
266.633327	8000.595455	9.886631	-0.055299	4.815629
266.670764	8000.528778	9.891635	-0.055306	4.815609
266.581712	8000.500621	9.896640	-0.055290	4.815601
266.885051	8000.407339	9.901645	-0.055346	4.815572
266.779005	8000.518877	9.906650	-0.055327	4.815606
266.875835	8000.571784	9.911655	-0.055345	4.815621
266.795791	8000.529884	9.916659	-0.055331	4.815609
266.652002	8000.459153	9.921664	-0.055304	4.815589
266.708347	8000.566956	9.926669	-0.055315	4.815620
266.835782	8000.565873	9.931674	-0.055339	4.815619
266.974889	8000.470953	9.936679	-0.055365	4.815591
266.752275	8000.608352	9.941683	-0.055324	4.815632
266.815063	8000.499352	9.946688	-0.055336	4.815600
266.756808	8000.542224	9.951693	-0.055325	4.815612
266.793871	8000.492637	9.956698	-0.055332	4.815598
267.001741	8000.459756	9.961703	-0.055371	4.815587
266.989944	8000.589944	9.966707	-0.055369	4.815625
266.810405	8000.441690	9.971712	-0.055336	4.815583
267.114545	8000.561056	9.976717	-0.055393	4.815616
266.890684	8000.523197	9.981722	-0.055352	4.815606
266.891783	8000.516826	9.986727	-0.055352	4.815604
266.915950	8000.603798	9.991731	-0.055357	4.815630
266.979689	8000.477717	9.996736	-0.055369	4.815592
266.919143	8000.523757	10.001741	-0.055358	4.815606
266.936174	8000.576418	10.006746	-0.055361	4.815621
267.213132	8000.482701	10.011751	-0.055413	4.815593
267.196623	8000.507028	10.016755	-0.055410	4.815600
267.123589	8000.550725	10.021760	-0.055397	4.815613
267.126199	8000.247332	10.026765	-0.055398	4.815524
267.003769	8000.488959	10.031770	-0.055375	4.815596
266.899044	8000.522517	10.036775	-0.055356	4.815606
266.951463	8000.509513	10.041779	-0.055366	4.815602
267.137743	8000.477344	10.046784	-0.055401	4.815592
267.004845	8000.476246	10.051789	-0.055376	4.815592
266.873875	8000.530742	10.056794	-0.055352	4.815608
266.910220	8000.469390	10.061799	-0.055359	4.815590
267.041633	8000.596595	10.066803	-0.055384	4.815627
266.984133	8000.468516	10.071808	-0.055374	4.815590
267.214237	8000.527894	10.076813	-0.055417	4.815606
267.308226	8000.501684	10.081818	-0.055434	4.815598
267.190729	8000.516867	10.086823	-0.055413	4.815603
267.243286	8000.569046	10.091827	-0.055423	4.815618
267.355803	8000.436288	10.096832	-0.055444	4.815578
267.495438	8000.467463	10.101837	-0.055470	4.815587
267.069305	8000.503204	10.106842	-0.055391	4.815599
267.070946	8000.394264	10.111847	-0.055392	4.815567
267.067532	8000.487192	10.116851	-0.055391	4.815595
267.053957	8000.489128	10.121856	-0.055389	4.815595
267.148264	8000.499254	10.126861	-0.055407	4.815598
267.092598	8000.468440	10.131866	-0.055397	4.815589
267.067171	8000.525745	10.136871	-0.055392	4.815606
267.068202	8000.493729	10.141875	-0.055393	4.815596
267.362683	8000.408848	10.146880	-0.055448	4.815570
267.363067	8000.539238	10.151885	-0.055448	4.815608
267.186162	8000.498947	10.156890	-0.055416	4.815597
267.172389	8000.505154	10.161895	-0.055413	4.815599
267.170378	8000.466677	10.166899	-0.055413	4.815588
267.236501	8000.452830	10.171904	-0.055426	4.815584
267.319854	8000.321729	10.176909	-0.055441	4.815545
267.347517	8000.525228	10.181914	-0.055447	4.815604
267.541327	8000.497458	10.186919	-0.055483	4.815595
267.279930	8000.495309	10.191923	-0.055435	4.815596
267.288353	8000.469826	10.196928	-0.055437	4.815588
267.465004	8000.486651	10.201933	-0.055470	4.815592
267.304188	8000.460516	10.206938	-0.055440	4.815586
267.415452	8000.498703	10.211943	-0.055461	4.815596
267.547221	8000.621642	10.216947	-0.055486	4.815631
267.413267	8000.488027	10.221952	-0.055461	4.815593
267.358309	8000.517063	10.226957	-0.055451	4.815602
267.353947	8000.513808	10.231962	-0.055451	4.815601
267.304363	8000.504466	10.236967	-0.055442	4.815598
267.260504	8000.535822	10.241971	-0.055434	4.815608
267.305936	8000.468207	10.246976	-0.055443	4.815588
267.454063	8000.565771	10.251981	-0.055470	4.815616
267.648692	8000.498479	10.256986	-0.055507	4.815595
267.537612	8000.476368	10.261991	-0.055486	4.815589
267.449055	8000.568963	10.266995	-0.055470	4.815616
267.320457	8000.521987	10.272000	-0.055447	4.815603
267.510753	8000.584985	10.277005	-0.055482	4.815621
267.493967	8000.516345	10.282010	-0.055479	4.815601
267.471623	8000.501040	10.287015	-0.055476	4.815596
267.563831	8000.497240	10.292019	-0.055493	4.815595
267.606340	8000.598406	10.297024	-0.055501	4.815624
267.674019	8000.364466	10.302029	-0.055514	4.815556
267.523308	8000.535108	10.307034	-0.055486	4.815606
267.429848	8000.606251	10.312039	-0.055469	4.815627
267.520439	8000.510530	10.317043	-0.055486	4.815599
267.551230	8000.516403	10.322048	-0.055492	4.815601
267.516839	8000.425033	10.327053	-0.055486	4.815574
267.622868	8000.596702	10.332058	-0.055506	4.815624
267.799321	8000.468202	10.337063	-0.055539	4.815585
267.860811	8000.498090	10.342067	-0.055551	4.815594
267.760487	8000.494321	10.347072	-0.055532	4.815593
267.716808	8000.511790	10.352077	-0.055525	4.815598
267.566227	8000.607636	10.357082	-0.055497	4.815627
267.495719	8000.408817	10.362087	-0.055484	4.815569
267.668456	8000.615778	10.367091	-0.055516	4.815629
267.750110	8000.468620	10.372096	-0.055532	4.815586
267.591318	8000.567536	10.377101	-0.055502	4.815615
267.539975	8000.484435	10.382106	-0.055493	4.815591
267.784671	8000.581455	10.387111	-0.055539	4.815618
267.675350	8000.490987	10.392115	-0.055519	4.815592
267.650772	8000.575019	10.397120	-0.055515	4.815617
267.768170	8000.500042	10.402125	-0.055537	4.815595
267.712441	8000.599590	10.407130	-0.055527	4.815624
267.669641	8000.433283	10.412135	-0.055519	4.815576
267.720705	8000.515356	10.417139	-0.055529	4.815599
267.642435	8000.557899	10.422144	-0.055514	4.815612
267.586514	8000.293073	10.427149	-0.055504	4.815535
267.710158	8000.544102	10.432154	-0.055527	4.815608
267.920712	8000.485620	10.437159	-0.055567	4.815590
267.597262	8000.427953	10.442163	-0.055507	4.815574
267.747428	8000.526619	10.447168	-0.055535	4.815602
267.886333	8000.384679	10.452173	-0.055561	4.815560
267.789505	8000.504919	10.457178	-0.055543	4.815596
267.638640	8000.532374	10.462183	-0.055516	4.815605
267.737951	8000.422906	10.467187	-0.055534	4.815572
267.717482	8000.463196	10.472192	-0.055531	4.815584
267.744879	8000.480767	10.477197	-0.055536	4.815589
267.634076	8000.544145	10.482202	-0.055516	4.815608
267.870116	8000.502111	10.487207	-0.055560	4.815595
268.011551	8000.557893	10.492211	-0.055587	4.815610
267.800441	8000.484980	10.497216	-0.055548	4.815590
267.955944	8000.488635	10.502221	-0.055577	4.815590
267.852053	8000.538235	10.507226	-0.055558	4.815605
267.801522	8000.507506	10.512231	-0.055549	4.815596
267.910024	8000.586253	10.517235	-0.055569	4.815619
267.853337	8000.555422	10.522240	-0.055559	4.815610
268.043729	8000.373725	10.527245	-0.055594	4.815556
267.837810	8000.531704	10.532250	-0.055556	4.815603
268.058109	8000.555661	10.537255	-0.055598	4.815609
268.028344	8000.527411	10.542259	-0.055592	4.815601
268.025203	8000.557301	10.547264	-0.055592	4.815610
268.052285	8000.477629	10.552269	-0.055597	4.815587
267.772937	8000.604478	10.557274	-0.055546	4.815625
267.911920	8000.440099	10.562279	-0.055572	4.815576
267.934718	8000.559106	10.567283	-0.055576	4.815611
268.094277	8000.451699	10.572288	-0.055606	4.815579
268.101978	8000.557636	10.577293	-0.055608	4.815610
268.041226	8000.550246	10.582298	-0.055597	4.815608
267.958547	8000.497615	10.587303	-0.055582	4.815593
267.976884	8000.484049	10.592307	-0.055585	4.815589
267.933688	8000.543198	10.597312	-0.055578	4.815606
268.252079	8000.438410	10.602317	-0.055637	4.815574
268.127961	8000.571024	10.607322	-0.055614	4.815613
267.951831	8000.548909	10.612327	-0.055582	4.815608
267.914087	8000.479922	10.617331	-0.055575	4.815588
267.970757	8000.554609	10.622336	-0.055586	4.815609
268.063997	8000.502742	10.627341	-0.055603	4.815594
267.832375	8000.519248	10.632346	-0.055560	4.815600
268.042491	8000.488542	10.637351	-0.055600	4.815590
268.109527	8000.475779	10.642355	-0.055613	4.815586
267.953385	8000.551231	10.647360	-0.055584	4.815608
268.018446	8000.504242	10.652365	-0.055596	4.815594
268.057358	8000.555129	10.657370	-0.055604	4.815609
268.086753	8000.473357	10.662375	-0.055609	4.815585
268.029979	8000.564340	10.667379	-0.055599	4.815612
268.104444	8000.487586	10.672384	-0.055613	4.815589
268.088549	8000.501238	10.677389	-0.055611	4.815593
267.922853	8000.566916	10.682394	-0.055580	4.815613
267.865473	8000.479441	10.687399	-0.055569	4.815588
267.937606	8000.469967	10.692403	-0.055583	4.815585
267.777819	8000.531469	10.697408	-0.055554	4.815603
267.900183	8000.399941	10.702413	-0.055577	4.815564
267.849083	8000.367065	10.707418	-0.055567	4.815555
267.856839	8000.359736	10.712423	-0.055569	4.815553
267.978627	8000.460072	10.717427	-0.055592	4.815582
268.053253	8000.501930	10.722432	-0.055606	4.815593
267.878122	8000.553562	10.727437	-0.055574	4.815609
267.838369	8000.527284	10.732442	-0.055567	4.815602
268.069390	8000.332366	10.737447	-0.055610	4.815544
268.147979	8000.521749	10.742451	-0.055625	4.815599
268.065712	8000.493702	10.747456	-0.055610	4.815591
268.141386	8000.400940	10.752461	-0.055624	4.815563
267.943748	8000.483188	10.757466	-0.055588	4.815588
267.968574	8000.389588	10.762471	-0.055592	4.815561
268.163859	8000.554182	10.767475	-0.055629	4.815608
268.094006	8000.564807	10.772480	-0.055616	4.815611
268.051198	8000.445515	10.777485	-0.055609	4.815577
267.857038	8000.612236	10.782490	-0.055573	4.815626
267.977642	8000.399469	10.787495	-0.055595	4.815564
268.107989	8000.397366	10.792499	-0.055620	4.815562
267.820747	8000.518742	10.797504	-0.055567	4.815599
268.075592	8000.403289	10.802509	-0.055614	4.815564
268.141988	8000.498439	10.807514	-0.055627	4.815592
268.133870	8000.475888	10.812519	-0.055626	4.815585
268.200610	8000.405419	10.817523	-0.055639	4.815564
268.139993	8000.486721	10.822528	-0.055628	4.815588
268.409198	8000.497594	10.827533	-0.055678	4.815590
268.283838	8000.618434	10.832538	-0.055655	4.815626
268.131797	8000.360565	10.837543	-0.055627	4.815552
268.305971	8000.486343	10.842547	-0.055659	4.815587
268.102948	8000.460579	10.847552	-0.055622	4.815581
268.266112	8000.520994	10.852557	-0.055653	4.815598
267.984805	8000.428757	10.857562	-0.055600	4.815572
268.073573	8000.479397	10.862567	-0.055617	4.815587
267.989993	8000.489796	10.867571	-0.055602	4.815590
268.003165	8000.581932	10.872576	-0.055605	4.815617
268.084691	8000.381342	10.877581	-0.055620	4.815558
267.935619	8000.390662	10.882586	-0.055593	4.815561
268.064641	8000.340453	10.887591	-0.055617	4.815546
268.128822	8000.537078	10.892595	-0.055629	4.815603
267.954724	8000.420965	10.897600	-0.055597	4.815570
268.168777	8000.597622	10.902605	-0.055637	4.815621
268.215353	8000.464843	10.907610	-0.055646	4.815582
268.305563	8000.545427	10.912615	-0.055663	4.815605
268.278477	8000.290688	10.917619	-0.055658	4.815530
268.174070	8000.510179	10.922624	-0.055639	4.815595
268.291902	8000.423455	10.927629	-0.055661	4.815569
268.201163	8000.615391	10.932634	-0.055645	4.815626
268.009838	8000.465866	10.937639	-0.055609	4.815583
268.319536	8000.494504	10.942643	-0.055667	4.815590
268.171792	8000.453622	10.947648	-0.055640	4.815578
268.208736	8000.498065	10.952653	-0.055647	4.815591
268.191781	8000.529865	10.957658	-0.055644	4.815601
267.964601	8000.452412	10.962663	-0.055602	4.815579
268.028101	8000.491950	10.967667	-0.055614	4.815590
268.118419	8000.586426	10.972672	-0.055631	4.815617
268.282356	8000.358344	10.977677	-0.055662	4.815550
268.183174	8000.604637	10.982682	-0.055644	4.815622
268.075189	8000.431910	10.987687	-0.055624	4.815572
268.312052	8000.551243	10.992691	-0.055668	4.815606
268.209827	8000.536757	10.997696	-0.055650	4.815602
268.350585	8000.292265	11.002701	-0.055676	4.815530
268.352081	8000.516709	11.007706	-0.055677	4.815596
268.243755	8000.493574	11.012711	-0.055657	4.815590
268.328130	8000.504605	11.017715	-0.055673	4.815592
268.325940	8000.509935	11.022720	-0.055673	4.815594
268.437406	8000.460505	11.027725	-0.055694	4.815579
268.304433	8000.458335	11.032730	-0.055669	4.815579
268.248363	8000.542918	11.037735	-0.055659	4.815604
268.280550	8000.501798	11.042739	-0.055665	4.815592
268.130666	8000.563463	11.047744	-0.055637	4.815611
268.245095	8000.490573	11.052749	-0.055659	4.815589
268.472243	8000.511439	11.057754	-0.055702	4.815594
268.552973	8000.508519	11.062759	-0.055717	4.815592
268.268201	8000.523080	11.067763	-0.055664	4.815598
268.245176	8000.462884	11.072768	-0.055660	4.815581
268.374198	8000.517393	11.077773	-0.055684	4.815596
268.426919	8000.485160	11.082778	-0.055694	4.815586
268.314010	8000.454470	11.087783	-0.055674	4.815578
268.337032	8000.509369	11.092787	-0.055678	4.815594
268.519821	8000.569040	11.097792	-0.055713	4.815610
268.479232	8000.392081	11.102797	-0.055705	4.815559
268.415442	8000.571639	11.107802	-0.055694	4.815611
268.447839	8000.500602	11.112807	-0.055700	4.815591
268.594659	8000.447481	11.117811	-0.055727	4.815574
268.300082	8000.538817	11.122816	-0.055673	4.815602
268.398940	8000.311798	11.127821	-0.055691	4.815536
268.365373	8000.366833	11.132826	-0.055685	4.815552
268.334119	8000.442208	11.137831	-0.055680	4.815574
268.424616	8000.522796	11.142835	-0.055697	4.815597
268.300989	8000.552837	11.147840	-0.055674	4.815606
268.604754	8000.539704	11.152845	-0.055731	4.815601
268.638741	8000.523190	11.157850	-0.055738	4.815596
268.588524	8000.440105	11.162855	-0.055729	4.815572
268.482186	8000.388152	11.167859	-0.055709	4.815557
268.252061	8000.493374	11.172864	-0.055666	4.815589
268.413499	8000.515293	11.177869	-0.055697	4.815595
268.380325	8000.480575	11.182874	-0.055691	4.815585
268.240871	8000.466544	11.187879	-0.055665	4.815582
268.334478	8000.489481	11.192883	-0.055683	4.815588
268.353694	8000.546455	11.197888	-0.055687	4.815604
268.406925	8000.518504	11.202893	-0.055697	4.815596
268.431335	8000.408868	11.207898	-0.055702	4.815564
268.560948	8000.489033	11.212903	-0.055726	4.815587
268.679970	8000.496362	11.217907	-0.055748	4.815588
268.369383	8000.543622	11.222912	-0.055691	4.815603
268.669260	8000.398991	11.227917	-0.055747	4.815560
268.793230	8000.557070	11.232922	-0.055770	4.815605
268.626572	8000.583196	11.237927	-0.055740	4.815614
268.753295	8000.396171	11.242931	-0.055763	4.815558
268.638896	8000.513987	11.247936	-0.055742	4.815593
268.630594	8000.379234	11.252941	-0.055741	4.815554
268.500227	8000.613260	11.257946	-0.055717	4.815623
268.508248	8000.440307	11.262951	-0.055719	4.815572
268.655773	8000.575266	11.267955	-0.055747	4.815611
268.444520	8000.468153	11.272960	-0.055707	4.815581
268.533465	8000.505974	11.277965	-0.055724	4.815592
268.633988	8000.603827	11.282970	-0.055743	4.815620
268.599721	8000.454753	11.287975	-0.055737	4.815576
268.681648	8000.334310	11.292979	-0.055753	4.815541
268.521502	8000.550748	11.297984	-0.055723	4.815605
268.707236	8000.487583	11.302989	-0.055758	4.815585
268.705281	8000.425597	11.307994	-0.055758	4.815567
268.778582	8000.411868	11.312999	-0.055772	4.815563
268.747627	8000.356884	11.318003	-0.055766	4.815547
268.565850	8000.481068	11.323008	-0.055733	4.815584
268.647175	8000.562575	11.328013	-0.055748	4.815607
268.715083	8000.510290	11.333018	-0.055761	4.815592
268.863438	8000.565120	11.338023	-0.055789	4.815607
268.861322	8000.496719	11.343027	-0.055789	4.815587
268.817415	8000.452206	11.348032	-0.055781	4.815574
268.938627	8000.612378	11.353037	-0.055804	4.815621
268.611794	8000.503357	11.358042	-0.055743	4.815590
268.527760	8000.478486	11.363047	-0.055728	4.815583
268.708973	8000.486840	11.368051	-0.055762	4.815585
268.585207	8000.511536	11.373056	-0.055739	4.815593
268.962945	8000.486801	11.378061	-0.055809	4.815584
268.774705	8000.481581	11.383066	-0.055775	4.815583
268.656077	8000.580094	11.388071	-0.055753	4.815612
268.858614	8000.379360	11.393075	-0.055791	4.815553
268.842558	8000.506278	11.398080	-0.055788	4.815590
268.799044	8000.491691	11.403085	-0.055780	4.815586
268.701740	8000.523235	11.408090	-0.055762	4.815596
268.694770	8000.524212	11.413095	-0.055761	4.815596
268.873139	8000.521834	11.418099	-0.055795	4.815594
268.508178	8000.445312	11.423104	-0.055727	4.815574
268.577303	8000.554400	11.428109	-0.055740	4.815605
268.762959	8000.483753	11.433114	-0.055775	4.815584
268.737947	8000.542135	11.438119	-0.055771	4.815601
268.854525	8000.559041	11.443123	-0.055793	4.815605
268.627008	8000.473031	11.448128	-0.055750	4.815581
268.639196	8000.502107	11.453133	-0.055753	4.815590
268.806641	8000.574349	11.458138	-0.055785	4.815610
268.662122	8000.450171	11.463143	-0.055758	4.815574
268.902065	8000.475522	11.468147	-0.055803	4.815581
268.804541	8000.510268	11.473152	-0.055785	4.815591
268.871248	8000.546654	11.478157	-0.055798	4.815601
268.857849	8000.558210	11.483162	-0.055795	4.815605
268.772707	8000.445697	11.488167	-0.055780	4.815572
268.926665	8000.598929	11.493171	-0.055809	4.815616
268.935529	8000.484760	11.498176	-0.055811	4.815583
269.049877	8000.472777	11.503181	-0.055832	4.815579
268.968669	8000.508861	11.508186	-0.055817	4.815590
268.673048	8000.516831	11.513191	-0.055762	4.815594
268.768238	8000.469269	11.518195	-0.055780	4.815579
268.853321	8000.570073	11.523200	-0.055797	4.815608
268.849322	8000.380892	11.528205	-0.055796	4.815553
268.677114	8000.600338	11.533210	-0.055764	4.815618
268.743742	8000.457202	11.538215	-0.055777	4.815576
268.666225	8000.442055	11.543219	-0.055763	4.815572
268.847041	8000.548712	11.548224	-0.055797	4.815602
269.048523	8000.544579	11.553229	-0.055834	4.815600
268.974400	8000.517733	11.558234	-0.055821	4.815592
268.895318	8000.410662	11.563239	-0.055806	4.815562
268.916708	8000.482632	11.568243	-0.055811	4.815582
268.882045	8000.469261	11.573248	-0.055804	4.815579
268.914247	8000.506146	11.578253	-0.055811	4.815589
269.023564	8000.471640	11.583258	-0.055831	4.815579
269.031291	8000.495300	11.588263	-0.055833	4.815586
268.698216	8000.522954	11.593267	-0.055771	4.815595
268.715950	8000.561739	11.598272	-0.055775	4.815606
268.944122	8000.357153	11.603277	-0.055817	4.815546
268.866646	8000.509773	11.608282	-0.055803	4.815591
268.649028	8000.499795	11.613287	-0.055763	4.815589
268.944807	8000.418141	11.618291	-0.055818	4.815563
268.862702	8000.576028	11.623296	-0.055803	4.815610
268.982607	8000.495748	11.628301	-0.055826	4.815586
269.136305	8000.378625	11.633306	-0.055855	4.815551
269.005803	8000.479079	11.638311	-0.055831	4.815581
269.075219	8000.355223	11.643315	-0.055844	4.815544
268.859745	8000.451070	11.648320	-0.055804	4.815573
269.057246	8000.499231	11.653325	-0.055841	4.815587
268.897365	8000.505165	11.658330	-0.055812	4.815589
268.837725	8000.554427	11.663335	-0.055801	4.815604
268.950055	8000.497531	11.668339	-0.055822	4.815587
269.023619	8000.551128	11.673344	-0.055836	4.815602
269.016420	8000.452723	11.678349	-0.055835	4.815573
268.926744	8000.468364	11.683354	-0.055818	4.815578
268.953673	8000.574620	11.688359	-0.055824	4.815609
269.064907	8000.479237	11.693363	-0.055845	4.815581
268.927480	8000.476993	11.698368	-0.055819	4.815581
268.959439	8000.568372	11.703373	-0.055826	4.815607
269.000238	8000.492130	11.708378	-0.055833	4.815585
269.058359	8000.443957	11.713383	-0.055844	4.815570
268.962549	8000.483006	11.718387	-0.055827	4.815582
268.844344	8000.490696	11.723392	-0.055805	4.815585
268.883570	8000.556549	11.728397	-0.055813	4.815604
268.931895	8000.553095	11.733402	-0.055822	4.815603
268.903634	8000.446862	11.738407	-0.055817	4.815572
269.134812	8000.506265	11.743411	-0.055860	4.815588
269.045741	8000.401166	11.748416	-0.055844	4.815558
268.956806	8000.519403	11.753421	-0.055828	4.815593
268.971422	8000.505775	11.758426	-0.055831	4.815589
268.965137	8000.468294	11.763431	-0.055830	4.815578
269.248062	8000.421692	11.768435	-0.055883	4.815563
269.183515	8000.570252	11.773440	-0.055871	4.815606
269.067282	8000.358915	11.778445	-0.055849	4.815545
269.212549	8000.345305	11.783450	-0.055877	4.815541
269.132685	8000.483995	11.788455	-0.055862	4.815582
269.269147	8000.374068	11.793459	-0.055888	4.815549
269.002892	8000.472283	11.798464	-0.055839	4.815579
269.190048	8000.444404	11.803469	-0.055874	4.815570
269.320088	8000.522442	11.808474	-0.055898	4.815592
269.116459	8000.452853	11.813479	-0.055860	4.815572
269.159600	8000.388404	11.818483	-0.055869	4.815553
269.057989	8000.505363	11.823488	-0.055850	4.815588
269.119730	8000.501062	11.828493	-0.055862	4.815587
269.123819	8000.575953	11.833498	-0.055863	4.815608
269.137297	8000.468271	11.838503	-0.055866	4.815577
269.146925	8000.420367	11.843507	-0.055868	4.815563
268.974728	8000.501967	11.848512	-0.055836	4.815587
269.101022	8000.557503	11.853517	-0.055860	4.815603
269.123074	8000.477745	11.858522	-0.055864	4.815580
269.195687	8000.466143	11.863527	-0.055878	4.815576
269.305529	8000.558808	11.868531	-0.055899	4.815602
269.016404	8000.447202	11.873536	-0.055845	4.815571
269.044359	8000.477607	11.878541	-0.055850	4.815580
269.246391	8000.578204	11.883546	-0.055888	4.815608
269.257336	8000.430942	11.888551	-0.055891	4.815565
269.176143	8000.492672	11.893555	-0.055876	4.815584
269.056580	8000.491791	11.898560	-0.055854	4.815584
269.096884	8000.571555	11.903565	-0.055862	4.815607
269.202119	8000.416231	11.908570	-0.055881	4.815561
269.146861	8000.455949	11.913575	-0.055871	4.815573
269.205930	8000.391762	11.918579	-0.055882	4.815554
269.343410	8000.589605	11.923584	-0.055908	4.815611
269.337933	8000.485884	11.928589	-0.055908	4.815581
269.289561	8000.519304	11.933594	-0.055899	4.815591
269.212009	8000.446452	11.938599	-0.055885	4.815570
269.365738	8000.485343	11.943603	-0.055914	4.815581
269.113065	8000.475854	11.948608	-0.055867	4.815579
269.046381	8000.441651	11.953613	-0.055855	4.815569
269.388630	8000.488995	11.958618	-0.055919	4.815582
269.363278	8000.472571	11.963623	-0.055914	4.815577
269.377003	8000.376647	11.968627	-0.055917	4.815549
269.396231	8000.497738	11.973632	-0.055921	4.815584
269.221976	8000.531218	11.978637	-0.055889	4.815595
269.204617	8000.446536	11.983642	-0.055886	4.815570
269.030467	8000.427657	11.988647	-0.055853	4.815565
269.293377	8000.560248	11.993651	-0.055903	4.815603
269.345080	8000.489528	11.998656	-0.055913	4.815582
269.197774	8000.420868	12.003661	-0.055885	4.815562
269.332331	8000.525696	12.008666	-0.055911	4.815592
269.098194	8000.452398	12.013671	-0.055867	4.815572
269.366972	8000.495324	12.018675	-0.055918	4.815583
269.433686	8000.484693	12.023680	-0.055930	4.815580
269.571787	8000.385478	12.028685	-0.055956	4.815550
269.410854	8000.347582	12.033690	-0.055927	4.815540
269.331454	8000.473457	12.038695	-0.055912	4.815577
269.395456	8000.511937	12.043699	-0.055924	4.815588
269.348439	8000.510115	12.048704	-0.055916	4.815588
269.365401	8000.380050	12.053709	-0.055919	4.815550
269.499891	8000.459230	12.058714	-0.055945	4.815572
269.241634	8000.503079	12.063719	-0.055897	4.815586
269.432581	8000.425039	12.068723	-0.055932	4.815562
269.275825	8000.518649	12.073728	-0.055904	4.815591
269.388488	8000.276893	12.078733	-0.055925	4.815519
269.248862	8000.401774	12.083738	-0.055899	4.815557
269.253217	8000.542922	12.088743	-0.055900	4.815598
269.370824	8000.467947	12.093747	-0.055922	4.815575
269.393906	8000.453390	12.098752	-0.055927	4.815571
269.266221	8000.459855	12.103757	-0.055903	4.815573
269.325469	8000.329419	12.108762	-0.055915	4.815535
269.272248	8000.483509	12.113767	-0.055905	4.815580
269.307032	8000.441363	12.118771	-0.055912	4.815568
269.396770	8000.477061	12.123776	-0.055929	4.815578
269.496732	8000.465910	12.128781	-0.055948	4.815574
269.483759	8000.497776	12.133786	-0.055945	4.815583
269.304141	8000.558951	12.138791	-0.055912	4.815602
269.609493	8000.377008	12.143795	-0.055969	4.815547
269.613650	8000.425186	12.148800	-0.055970	4.815562
269.469989	8000.445280	12.153805	-0.055944	4.815568
269.686504	8000.382622	12.158810	-0.055984	4.815549
269.449212	8000.559322	12.163815	-0.055941	4.815601
269.493539	8000.298271	12.168819	-0.055949	4.815525
269.248272	8000.448125	12.173824	-0.055904	4.815570
269.495487	8000.402002	12.178829	-0.055950	4.815555
269.481942	8000.515073	12.183834	-0.055948	4.815588
269.218494	8000.387861	12.188839	-0.055899	4.815552
269.288932	8000.406144	12.193843	-0.055912	4.815557
269.351836	8000.406135	12.198848	-0.055924	4.815557
269.475252	8000.468036	12.203853	-0.055947	4.815575
269.471838	8000.388926	12.208858	-0.055947	4.815552
269.483513	8000.519510	12.213863	-0.055949	4.815590
269.242841	8000.494190	12.218867	-0.055905	4.815583
269.335778	8000.446591	12.223872	-0.055922	4.815569
269.422234	8000.394611	12.228877	-0.055939	4.815553
269.465817	8000.518241	12.233882	-0.055947	4.815589
269.501069	8000.469690	12.238887	-0.055954	4.815575
269.518776	8000.313991	12.243891	-0.055957	4.815529
269.402959	8000.365533	12.248896	-0.055936	4.815545
269.368254	8000.326514	12.253901	-0.055930	4.815534
269.457007	8000.299149	12.258906	-0.055947	4.815525
269.491429	8000.315768	12.263911	-0.055953	4.815530
269.398353	8000.194575	12.268915	-0.055936	4.815495
269.475910	8000.476915	12.273920	-0.055951	4.815577
269.572309	8000.375944	12.278925	-0.055969	4.815547
269.637070	8000.414436	12.283930	-0.055982	4.815558
269.378982	8000.395240	12.288935	-0.055934	4.815554
269.393288	8000.500221	12.293939	-0.055937	4.815584
269.439108	8000.493520	12.298944	-0.055946	4.815582
269.551599	8000.360756	12.303949	-0.055967	4.815543
269.596626	8000.236497	12.308954	-0.055975	4.815506
269.557907	8000.513715	12.313959	-0.055969	4.815587
269.610557	8000.329739	12.318963	-0.055978	4.815533
269.451522	8000.475673	12.323968	-0.055949	4.815577
269.513577	8000.456416	12.328973	-0.055961	4.815571
269.591994	8000.373314	12.333978	-0.055976	4.815546
269.381341	8000.506642	12.338983	-0.055937	4.815586
269.452231	8000.380671	12.343987	-0.055950	4.815549
269.394500	8000.423554	12.348992	-0.055940	4.815562
269.270988	8000.308269	12.353997	-0.055917	4.815529
269.367911	8000.566353	12.359002	-0.055935	4.815604
269.620301	8000.478641	12.364007	-0.055983	4.815577
269.698344	8000.427590	12.369011	-0.055997	4.815562
269.365493	8000.473414	12.374016	-0.055936	4.815577
269.570070	8000.460783	12.379021	-0.055974	4.815572
269.803609	8000.287272	12.384026	-0.056018	4.815520
269.558448	8000.526890	12.389031	-0.055972	4.815591
269.583976	8000.314684	12.394035	-0.055977	4.815529
269.515523	8000.501650	12.399040	-0.055965	4.815584
269.687964	8000.366669	12.404045	-0.055997	4.815544
269.614859	8000.408229	12.409050	-0.055984	4.815556
269.563134	8000.493955	12.414055	-0.055975	4.815582
269.595781	8000.388726	12.419059	-0.055981	4.815551
269.438063	8000.405381	12.424064	-0.055952	4.815556
269.641948	8000.493187	12.429069	-0.055990	4.815581
269.683554	8000.201102	12.434074	-0.055998	4.815495
269.609158	8000.424301	12.439079	-0.055984	4.815561
269.465433	8000.327917	12.444083	-0.055958	4.815533
269.670067	8000.553585	12.449088	-0.055996	4.815598
269.540821	8000.392253	12.454093	-0.055972	4.815552
269.453442	8000.387629	12.459098	-0.055956	4.815551
269.588812	8000.522391	12.464103	-0.055982	4.815590
269.590389	8000.371768	12.469107	-0.055982	4.815546
269.420098	8000.545300	12.474112	-0.055951	4.815597
269.468942	8000.438200	12.479117	-0.055960	4.815566
269.771675	8000.465658	12.484122	-0.056017	4.815572
269.524967	8000.458405	12.489127	-0.055971	4.815571
269.664898	8000.479971	12.494131	-0.055998	4.815577
269.689936	8000.377822	12.499136	-0.056003	4.815547
269.420482	8000.484533	12.504141	-0.055953	4.815579
269.464993	8000.507731	12.509146	-0.055961	4.815586
269.436048	8000.417514	12.514151	-0.055956	4.815560
269.444994	8000.294797	12.519155	-0.055958	4.815524
269.569338	8000.465709	12.524160	-0.055981	4.815573
269.663783	8000.271737	12.529165	-0.055999	4.815516
269.801259	8000.388367	12.534170	-0.056025	4.815549
269.707773	8000.437072	12.539175	-0.056008	4.815564
269.609616	8000.345713	12.544179	-0.055990	4.815538
269.549246	8000.476177	12.549184	-0.055979	4.815576
269.652561	8000.465082	12.554189	-0.055998	4.815572
269.602385	8000.400161	12.559194	-0.055989	4.815554
269.521717	8000.581583	12.564199	-0.055975	4.815607
269.777987	8000.365703	12.569203	-0.056023	4.815543
269.654958	8000.523986	12.574208	-0.056000	4.815590
269.572440	8000.402964	12.579213	-0.055985	4.815555
269.680554	8000.488122	12.584218	-0.056005	4.815579
269.545104	8000.572466	12.589223	-0.055980	4.815604
269.627345	8000.279982	12.594227	-0.055996	4.815518
269.707656	8000.493980	12.599232	-0.056011	4.815581
269.744521	8000.560865	12.604237	-0.056018	4.815600
269.803709	8000.387682	12.609242	-0.056029	4.815549
269.713041	8000.469560	12.614247	-0.056013	4.815573
269.827691	8000.423388	12.619251	-0.056034	4.815559
269.825209	8000.392380	12.624256	-0.056034	4.815550
269.806473	8000.469033	12.629261	-0.056031	4.815573
269.969401	8000.372364	12.634266	-0.056062	4.815544
269.620507	8000.473491	12.639271	-0.055997	4.815575
269.625127	8000.351769	12.644275	-0.055998	4.815539
269.726376	8000.496655	12.649280	-0.056017	4.815581
269.691660	8000.445881	12.654285	-0.056011	4.815567
269.697489	8000.367992	12.659290	-0.056012	4.815544
269.740410	8000.486269	12.664295	-0.056021	4.815578
269.747403	8000.405194	12.669299	-0.056022	4.815554
269.757824	8000.504769	12.674304	-0.056024	4.815583
269.627052	8000.502634	12.679309	-0.056000	4.815583
269.664650	8000.090801	12.684314	-0.056007	4.815463
269.978416	8000.334295	12.689319	-0.056066	4.815532
269.724309	8000.397447	12.694323	-0.056019	4.815552
269.701917	8000.403512	12.699328	-0.056015	4.815554
269.892019	8000.462239	12.704333	-0.056051	4.815570
269.782511	8000.350389	12.709338	-0.056031	4.815538
269.781099	8000.537394	12.714343	-0.056031	4.815593
269.711391	8000.371702	12.719347	-0.056018	4.815545
269.672573	8000.340095	12.724352	-0.056011	4.815536
269.615568	8000.459929	12.729357	-0.056001	4.815571
269.777084	8000.190125	12.734362	-0.056031	4.815491
269.767233	8000.385538	12.739367	-0.056029	4.815548
269.749152	8000.252756	12.744371	-0.056026	4.815510
269.675280	8000.423605	12.749376	-0.056013	4.815560
269.740793	8000.389445	12.754381	-0.056025	4.815550
269.698136	8000.354568	12.759386	-0.056017	4.815540
269.607426	8000.478121	12.764391	-0.056001	4.815576
269.819828	8000.392954	12.769395	-0.056041	4.815550
269.820886	8000.390858	12.774400	-0.056041	4.815550
269.543973	8000.405546	12.779405	-0.055990	4.815555
269.807437	8000.365035	12.784410	-0.056039	4.815542
269.697080	8000.473303	12.789415	-0.056019	4.815574
269.572539	8000.352656	12.794419	-0.055996	4.815540
269.566834	8000.433799	12.799424	-0.055995	4.815563
269.891856	8000.440253	12.804429	-0.056056	4.815564
270.018457	8000.385729	12.809434	-0.056080	4.815547
269.940086	8000.374841	12.814439	-0.056065	4.815544
269.970244	8000.336892	12.819443	-0.056071	4.815533
269.989243	8000.485765	12.824448	-0.056075	4.815577
269.908436	8000.497277	12.829453	-0.056060	4.815580
269.925245	8000.238976	12.834458	-0.056064	4.815505
270.002525	8000.428348	12.839463	-0.056078	4.815560
269.930504	8000.339556	12.844467	-0.056065	4.815534
269.655736	8000.385270	12.849472	-0.056014	4.815549
269.641820	8000.484443	12.854477	-0.056012	4.815578
269.850806	8000.312664	12.859482	-0.056051	4.815527
269.749423	8000.364444	12.864487	-0.056032	4.815542
269.746573	8000.266109	12.869491	-0.056032	4.815513
269.965993	8000.391572	12.874496	-0.056073	4.815549
270.010144	8000.382706	12.879501	-0.056082	4.815546
269.922249	8000.263733	12.884506	-0.056066	4.815512
270.095147	8000.402321	12.889511	-0.056098	4.815552
269.943091	8000.313278	12.894515	-0.056070	4.815526
269.984530	8000.368483	12.899520	-0.056078	4.815542
269.937557	8000.383760	12.904525	-0.056070	4.815547
269.860713	8000.385721	12.909530	-0.056056	4.815548
269.700167	8000.514533	12.914535	-0.056026	4.815586
269.774463	8000.358697	12.919539	-0.056040	4.815540
269.993928	8000.418977	12.924544	-0.056081	4.815557
269.937468	8000.367844	12.929549	-0.056071	4.815542
269.999613	8000.255620	12.934554	-0.056083	4.815509
269.902534	8000.395097	12.939559	-0.056065	4.815550
269.920500	8000.360152	12.944563	-0.056068	4.815540
269.834891	8000.388683	12.949568	-0.056053	4.815549
269.805744	8000.460890	12.954573	-0.056048	4.815570
269.923029	8000.388046	12.959578	-0.056070	4.815548
270.022969	8000.301024	12.964583	-0.056089	4.815522
270.092190	8000.255171	12.969587	-0.056102	4.815508
270.146948	8000.269989	12.974592	-0.056112	4.815513
269.873789	8000.372365	12.979597	-0.056062	4.815544
269.952617	8000.201644	12.984602	-0.056076	4.815493
269.942489	8000.416288	12.989607	-0.056075	4.815556
269.937978	8000.306171	12.994611	-0.056074	4.815524
269.849222	8000.358159	12.999616	-0.056058	4.815540
269.861585	8000.366935	13.004621	-0.056061	4.815542
270.209504	8000.396208	13.009626	-0.056126	4.815549
270.031319	8000.377262	13.014631	-0.056093	4.815544
269.906876	8000.408358	13.019635	-0.056070	4.815554
270.107616	8000.234305	13.024640	-0.056107	4.815502
270.156892	8000.445657	13.029645	-0.056117	4.815564
270.182017	8000.393732	13.034650	-0.056122	4.815548
270.159220	8000.328193	13.039655	-0.056118	4.815529
270.115271	8000.220631	13.044659	-0.056110	4.815498
269.978193	8000.261136	13.049664	-0.056085	4.815511
269.965798	8000.420176	13.054669	-0.056083	4.815557
270.039083	8000.283558	13.059674	-0.056096	4.815517
270.002848	8000.330002	13.064679	-0.056090	4.815531
269.899556	8000.193677	13.069683	-0.056071	4.815491
269.942518	8000.262799	13.074688	-0.056079	4.815511
269.924845	8000.477320	13.079693	-0.056076	4.815574
269.958065	8000.253484	13.084698	-0.056083	4.815508
269.868504	8000.452926	13.089703	-0.056066	4.815567
270.136470	8000.241512	13.094707	-0.056116	4.815504
269.983558	8000.389686	13.099712	-0.056088	4.815548
269.930912	8000.326861	13.104717	-0.056079	4.815530
269.983521	8000.266841	13.109722	-0.056089	4.815512
269.790764	8000.429317	13.114727	-0.056053	4.815561
269.792528	8000.150465	13.119731	-0.056054	4.815479
270.078911	8000.433049	13.124736	-0.056107	4.815560
270.128564	8000.364432	13.129741	-0.056117	4.815540
270.069822	8000.232047	13.134746	-0.056106	4.815502
270.149702	8000.516570	13.139751	-0.056121	4.815584
270.116651	8000.304462	13.144755	-0.056115	4.815523
269.976082	8000.347047	13.149760	-0.056089	4.815536
269.920798	8000.446606	13.154765	-0.056079	4.815565
269.928086	8000.116552	13.159770	-0.056081	4.815468
269.821670	8000.416164	13.164775	-0.056061	4.815557
269.875398	8000.313419	13.169779	-0.056072	4.815526
269.840439	8000.362020	13.174784	-0.056065	4.815541
269.901443	8000.343815	13.179789	-0.056077	4.815535
269.947712	8000.365973	13.184794	-0.056086	4.815541
269.825652	8000.359708	13.189799	-0.056063	4.815540
269.959255	8000.295682	13.194803	-0.056089	4.815521
270.152088	8000.367278	13.199808	-0.056125	4.815541
270.026477	8000.372708	13.204813	-0.056102	4.815543
270.151045	8000.299984	13.209818	-0.056125	4.815521
269.940115	8000.400181	13.214823	-0.056086	4.815551
269.944750	8000.386388	13.219827	-0.056087	4.815547
270.207024	8000.476229	13.224832	-0.056136	4.815572
270.247328	8000.458750	13.229837	-0.056144	4.815567
270.294877	8000.220189	13.234842	-0.056153	4.815497
270.042006	8000.387016	13.239847	-0.056106	4.815547
269.927536	8000.420414	13.244851	-0.056085	4.815557
269.988052	8000.331672	13.249856	-0.056097	4.815531
269.789921	8000.390405	13.254861	-0.056060	4.815549
270.038980	8000.453312	13.259866	-0.056107	4.815566
269.997041	8000.400280	13.264871	-0.056099	4.815551
269.935765	8000.190915	13.269875	-0.056088	4.815490
270.068312	8000.203810	13.274880	-0.056113	4.815493
270.009776	8000.341786	13.279885	-0.056102	4.815534
270.108249	8000.344502	13.284890	-0.056121	4.815534
270.067811	8000.416523	13.289895	-0.056114	4.815555
270.222067	8000.162626	13.294899	-0.056143	4.815480
270.123884	8000.243311	13.299904	-0.056125	4.815504
269.957470	8000.416908	13.304909	-0.056094	4.815556
270.087393	8000.243823	13.309914	-0.056118	4.815505
270.014696	8000.378360	13.314919	-0.056105	4.815544
269.920404	8000.365072	13.319923	-0.056088	4.815541
270.134906	8000.091866	13.324928	-0.056128	4.815460
270.036019	8000.328555	13.329933	-0.056110	4.815530
270.128552	8000.142031	13.334938	-0.056127	4.815475
270.047311	8000.255054	13.339943	-0.056112	4.815508
270.104587	8000.119241	13.344947	-0.056123	4.815468
270.120105	8000.229586	13.349952	-0.056126	4.815500
270.171098	8000.421731	13.354957	-0.056136	4.815556
270.261296	8000.400802	13.359962	-0.056153	4.815550
270.072337	8000.241689	13.364967	-0.056118	4.815504
270.049571	8000.257365	13.369971	-0.056114	4.815509
270.310658	8000.356803	13.374976	-0.056163	4.815537
270.235569	8000.343832	13.379981	-0.056150	4.815533
270.176224	8000.233877	13.384986	-0.056139	4.815501
270.244612	8000.186941	13.389991	-0.056152	4.815487
270.315735	8000.278970	13.394995	-0.056165	4.815514
270.208483	8000.203489	13.400000	-0.056145	4.815492
269.970888	8000.332098	13.405005	-0.056102	4.815531
270.038389	8000.254158	13.410010	-0.056114	4.815508
270.213165	8000.215389	13.415015	-0.056147	4.815496
270.136287	8000.376572	13.420019	-0.056133	4.815543
270.150802	8000.144947	13.425024	-0.056136	4.815475
270.012258	8000.305111	13.430029	-0.056111	4.815523
270.114839	8000.047157	13.435034	-0.056130	4.815447
270.244878	8000.155116	13.440039	-0.056154	4.815478
270.380898	8000.126394	13.445043	-0.056180	4.815469
270.393647	8000.114873	13.450048	-0.056182	4.815465
270.275252	8000.364065	13.455053	-0.056161	4.815539
269.999213	7999.881871	13.460058	-0.056109	4.815399
270.131687	8000.222822	13.465063	-0.056135	4.815498
270.279353	8000.115216	13.470067	-0.056162	4.815466
270.215697	8000.203951	13.475072	-0.056151	4.815492
270.206026	8000.355557	13.480077	-0.056149	4.815537
270.184483	8000.321028	13.485082	-0.056145	4.815527
270.178643	8000.320955	13.490087	-0.056145	4.815527
270.149915	8000.183722	13.495091	-0.056139	4.815487
270.236315	8000.267453	13.500096	-0.056156	4.815511
270.062576	8000.415283	13.505101	-0.056124	4.815555
269.940483	8000.373753	13.510106	-0.056101	4.815543
270.131505	8000.341664	13.515111	-0.056137	4.815533
270.039534	8000.309179	13.520115	-0.056120	4.815524
270.054225	8000.274180	13.525120	-0.056123	4.815513
270.210431	8000.241517	13.530125	-0.056153	4.815503
270.234901	8000.197062	13.535130	-0.056157	4.815490
270.256973	8000.269046	13.540135	-0.056162	4.815511
270.213736	8000.369873	13.545139	-0.056154	4.815541
270.234284	8000.293295	13.550144	-0.056158	4.815518
269.916676	8000.407761	13.555149	-0.056099	4.815553
270.015246	8000.397656	13.560154	-0.056118	4.815550
270.263321	8000.494743	13.565159	-0.056164	4.815577
270.217808	8000.205489	13.570163	-0.056156	4.815493
269.953858	8000.086817	13.575168	-0.056107	4.815459
269.905913	8000.290151	13.580173	-0.056098	4.815519
270.081389	8000.186209	13.585178	-0.056131	4.815488
270.200943	8000.333535	13.590183	-0.056154	4.815530
270.150442	8000.398979	13.595187	-0.056145	4.815549
270.331880	8000.350702	13.600192	-0.056179	4.815534
270.127124	8000.408257	13.605197	-0.056141	4.815552
270.102759	8000.379025	13.610202	-0.056137	4.815544
270.191405	8000.420050	13.615207	-0.056154	4.815555
270.016259	8000.348791	13.620211	-0.056121	4.815535
270.207490	8000.219462	13.625216	-0.056157	4.815497
270.307568	8000.407075	13.630221	-0.056176	4.815551
270.375805	8000.066269	13.635226	-0.056189	4.815451
270.402881	8000.400145	13.640231	-0.056194	4.815548
270.230804	8000.380230	13.645235	-0.056162	4.815543
270.223299	8000.391884	13.650240	-0.056161	4.815547
270.043011	8000.345118	13.655245	-0.056128	4.815534
270.169798	8000.252127	13.660250	-0.056152	4.815506
270.346094	8000.318107	13.665255	-0.056185	4.815525
270.348144	8000.361977	13.670259	-0.056185	4.815537
270.263215	8000.166111	13.675264	-0.056170	4.815481
270.235966	8000.377270	13.680269	-0.056165	4.815542
270.430876	8000.274716	13.685274	-0.056202	4.815512
270.166804	8000.430673	13.690279	-0.056153	4.815558
270.079788	8000.427123	13.695283	-0.056137	4.815558
270.328468	8000.074334	13.700288	-0.056183	4.815454
270.409996	8000.337511	13.705293	-0.056199	4.815530
270.295653	8000.222374	13.710298	-0.056178	4.815497
270.255656	8000.228149	13.715303	-0.056171	4.815499
270.243683	8000.356208	13.720307	-0.056169	4.815536
270.150911	8000.342945	13.725312	-0.056152	4.815533
270.107139	8000.372166	13.730317	-0.056144	4.815542
270.266736	8000.358794	13.735322	-0.056174	4.815537
270.327728	8000.358755	13.740327	-0.056185	4.815537
270.270566	8000.403785	13.745331	-0.056175	4.815550
270.412319	8000.346305	13.750336	-0.056202	4.815532
270.330827	8000.343914	13.755341	-0.056187	4.815532
270.227015	8000.311234	13.760346	-0.056168	4.815523
270.377645	8000.352213	13.765351	-0.056196	4.815534
270.399597	8000.406029	13.770355	-0.056200	4.815550
270.441199	8000.115006	13.775360	-0.056208	4.815465
270.365804	8000.361704	13.780365	-0.056194	4.815537
270.446735	8000.256200	13.785370	-0.056210	4.815506
270.279490	8000.307962	13.790375	-0.056179	4.815522
270.160989	8000.310304	13.795379	-0.056157	4.815523
270.388001	8000.122792	13.800384	-0.056199	4.815467
270.261432	8000.319488	13.805389	-0.056176	4.815525
270.085153	8000.340111	13.810394	-0.056144	4.815532
270.317165	8000.288395	13.815399	-0.056187	4.815516
270.239517	8000.355528	13.820403	-0.056173	4.815536
270.226791	8000.346792	13.825408	-0.056171	4.815533
270.099436	8000.483633	13.830413	-0.056148	4.815574
270.362836	8000.386484	13.835418	-0.056197	4.815544
270.355919	8000.365021	13.840423	-0.056196	4.815538
270.242927	8000.335395	13.845427	-0.056175	4.815530
270.477820	8000.193962	13.850432	-0.056219	4.815488
270.168409	8000.339554	13.855437	-0.056162	4.815532
270.382578	8000.273651	13.860442	-0.056202	4.815511
270.293051	8000.343794	13.865447	-0.056185	4.815532
270.354664	8000.360863	13.870451	-0.056197	4.815537
270.312059	8000.400790	13.875456	-0.056189	4.815549
270.365054	8000.365355	13.880461	-0.056199	4.815538
270.650770	8000.254682	13.885466	-0.056253	4.815504
270.105827	8000.462641	13.890471	-0.056152	4.815568
270.057301	8000.382785	13.895475	-0.056143	4.815545
270.193455	8000.233312	13.900480	-0.056168	4.815500
270.070749	8000.464267	13.905485	-0.056146	4.815568
270.080380	8000.265687	13.910490	-0.056148	4.815510
270.128581	8000.364818	13.915495	-0.056157	4.815539
270.283481	8000.301143	13.920499	-0.056186	4.815520
270.430541	8000.269397	13.925504	-0.056214	4.815510
270.117930	8000.505768	13.930509	-0.056156	4.815580
270.381899	8000.403286	13.935514	-0.056205	4.815549
270.445447	8000.256888	13.940519	-0.056217	4.815506
270.328967	8000.265675	13.945523	-0.056196	4.815509
270.364230	8000.221398	13.950528	-0.056203	4.815496
270.296342	8000.523789	13.955533	-0.056191	4.815585
270.328723	8000.217652	13.960538	-0.056197	4.815495
270.512852	8000.455811	13.965543	-0.056231	4.815564
270.353480	8000.376262	13.970547	-0.056202	4.815541
270.522879	8000.354502	13.975552	-0.056234	4.815534
270.379278	8000.394900	13.980557	-0.056207	4.815547
270.484546	8000.214995	13.985562	-0.056227	4.815493
270.388021	8000.353413	13.990567	-0.056209	4.815534
270.177786	8000.262340	13.995571	-0.056170	4.815509
270.356706	8000.372178	14.000576	-0.056204	4.815540
270.272029	8000.411410	14.005581	-0.056189	4.815552
270.126915	8000.292559	14.010586	-0.056162	4.815518
270.083364	8000.378421	14.015591	-0.056154	4.815543
270.260685	8000.368547	14.020595	-0.056187	4.815539
270.411895	8000.386026	14.025600	-0.056216	4.815544
270.299135	8000.387394	14.030605	-0.056195	4.815545
270.388207	8000.373926	14.035610	-0.056212	4.815540
270.485725	8000.312510	14.040615	-0.056230	4.815522
270.378945	8000.102391	14.045619	-0.056210	4.815461
270.382319	8000.216811	14.050624	-0.056211	4.815494
270.364407	8000.394997	14.055629	-0.056208	4.815547
270.361015	8000.144908	14.060634	-0.056208	4.815473
270.233117	8000.376847	14.065639	-0.056184	4.815542
270.214000	8000.330604	14.070643	-0.056181	4.815528
270.340225	8000.143565	14.075648	-0.056205	4.815473
270.098413	8000.331948	14.080653	-0.056160	4.815529
270.204639	8000.155265	14.085658	-0.056180	4.815477
270.593264	8000.261083	14.090663	-0.056253	4.815506
270.335179	8000.360502	14.095667	-0.056205	4.815537
270.310261	8000.122881	14.100672	-0.056200	4.815467
270.243716	8000.408195	14.105677	-0.056189	4.815551
270.609980	8000.390754	14.110682	-0.056257	4.815544
270.521380	8000.195893	14.115687	-0.056241	4.815488
270.473997	8000.455879	14.120691	-0.056232	4.815564
270.340133	8000.311565	14.125696	-0.056207	4.815522
270.469088	8000.422716	14.130701	-0.056232	4.815554
270.509770	8000.192588	14.135706	-0.056239	4.815487
270.437147	8000.223470	14.140711	-0.056226	4.815496
270.494468	8000.157116	14.145715	-0.056237	4.815476
270.288149	8000.377075	14.150720	-0.056199	4.815542
270.229560	8000.260721	14.155725	-0.056188	4.815508
270.532375	8000.339476	14.160730	-0.056245	4.815529
270.381734	8000.205572	14.165735	-0.056217	4.815491
270.449366	8000.329603	14.170739	-0.056230	4.815527
270.685248	8000.242686	14.175744	-0.056274	4.815500
270.427799	8000.347459	14.180749	-0.056227	4.815532
270.560859	8000.348610	14.185754	-0.056252	4.815532
270.597013	8000.379151	14.190759	-0.056259	4.815541
270.674064	8000.334495	14.195763	-0.056273	4.815527
270.619573	8000.252403	14.200768	-0.056263	4.815503
270.654455	8000.272236	14.205773	-0.056270	4.815509
270.618571	8000.360363	14.210778	-0.056264	4.815535
270.684222	8000.219342	14.215783	-0.056276	4.815493
270.639982	8000.367174	14.220787	-0.056268	4.815537
270.707161	8000.156718	14.225792	-0.056281	4.815475
270.437182	8000.218540	14.230797	-0.056231	4.815494
270.365169	8000.067769	14.235802	-0.056218	4.815451
270.349815	7999.537519	14.240807	-0.056215	4.815296

270.594435	7996.280603	14.245811	-0.056258	4.814343
270.392128	7990.698212	14.250816	-0.056217	4.812712
270.149251	7983.915013	14.255821	-0.056168	4.810730
270.395318	7976.659093	14.260826	-0.056209	4.808607
270.186963	7969.017300	14.265831	-0.056166	4.806371
270.135980	7961.173710	14.270835	-0.056151	4.804075
270.353484	7953.365727	14.275840	-0.056187	4.801787
270.418114	7945.387600	14.280845	-0.056194	4.799449
270.297518	7937.432924	14.285850	-0.056167	4.797117
270.186660	7929.413154	14.290855	-0.056141	4.794765
270.036802	7921.368087	14.295859	-0.056108	4.792404
270.249315	7913.391792	14.300864	-0.056143	4.790061
269.984736	7905.383864	14.305869	-0.056089	4.787710
270.125570	7897.422826	14.310874	-0.056110	4.785369
269.926227	7889.406807	14.315879	-0.056068	4.783012
269.698019	7881.389124	14.320883	-0.056020	4.780654
269.983221	7873.438586	14.325888	-0.056069	4.778313
269.846527	7865.367561	14.330893	-0.056038	4.775936
269.850111	7857.390364	14.335898	-0.056034	4.773586
269.876172	7849.346455	14.340903	-0.056034	4.771214
269.829515	7841.344777	14.345907	-0.056020	4.768854
269.875479	7833.392664	14.350912	-0.056024	4.766508
269.639487	7825.353253	14.355917	-0.055975	4.764135
269.749809	7817.411942	14.360922	-0.055990	4.761789
269.638832	7809.358876	14.365927	-0.055965	4.759409
269.599824	7801.409955	14.370931	-0.055953	4.757059
269.681065	7793.371412	14.375936	-0.055963	4.754681
269.270967	7785.359788	14.380941	-0.055881	4.752311
269.411911	7777.277287	14.385946	-0.055903	4.749917
269.357946	7769.372619	14.390951	-0.055888	4.747575
269.222011	7761.264622	14.395955	-0.055857	4.745172
269.172738	7753.396394	14.400960	-0.055843	4.742839
269.141356	7745.327129	14.405965	-0.055833	4.740444
269.076390	7737.286854	14.410970	-0.055815	4.738057
268.986850	7729.329231	14.415975	-0.055794	4.735694
268.977995	7721.268228	14.420979	-0.055787	4.733299
269.101335	7713.350101	14.425984	-0.055805	4.730944
268.983551	7705.325546	14.430989	-0.055778	4.728557
268.830619	7697.320506	14.435994	-0.055745	4.726175
268.918397	7689.300764	14.440999	-0.055756	4.723787
268.894698	7681.341694	14.446003	-0.055747	4.721416
268.911805	7673.303221	14.451008	-0.055745	4.719020
268.640954	7665.365841	14.456013	-0.055690	4.716653
268.624148	7657.293422	14.461018	-0.055682	4.714244
268.750604	7649.278566	14.466023	-0.055700	4.711851
268.606608	7641.235324	14.471027	-0.055668	4.709449
268.697503	7633.260705	14.476032	-0.055680	4.707066
268.575785	7625.282256	14.481037	-0.055653	4.704681
268.430091	7617.365121	14.486042	-0.055621	4.702313
268.534090	7609.314053	14.491047	-0.055635	4.699903
268.563533	7601.329111	14.496051	-0.055636	4.697512
268.554357	7593.307344	14.501056	-0.055629	4.695108
268.446629	7585.276566	14.506061	-0.055604	4.692701
268.467576	7577.241397	14.511066	-0.055603	4.690291
268.480534	7569.288322	14.516071	-0.055600	4.687905
268.143971	7561.210412	14.521075	-0.055533	4.685480
268.274700	7553.336903	14.526080	-0.055552	4.683115
268.209243	7545.332276	14.531085	-0.055535	4.680710
267.960686	7537.334981	14.536090	-0.055484	4.678305
268.095944	7529.312733	14.541095	-0.055504	4.675892
268.053174	7521.233566	14.546099	-0.055491	4.673460
267.998191	7513.155462	14.551104	-0.055476	4.671027
267.876204	7505.164164	14.556109	-0.055448	4.668620
267.857204	7497.172311	14.561114	-0.055440	4.666211
267.975656	7489.258639	14.566119	-0.055457	4.663823
267.634541	7481.201341	14.571123	-0.055388	4.661392
267.698661	7473.249140	14.576128	-0.055395	4.658991
267.480431	7465.277289	14.581133	-0.055350	4.656583
267.586212	7457.226063	14.586138	-0.055364	4.654150
267.492830	7449.213478	14.591143	-0.055342	4.651727
267.465675	7441.171267	14.596147	-0.055332	4.649293
267.577608	7433.263579	14.601152	-0.055348	4.646899
267.573607	7425.208150	14.606157	-0.055342	4.644460
267.600010	7417.268270	14.611162	-0.055342	4.642053
267.808655	7409.237169	14.616167	-0.055376	4.639618
267.297177	7401.245811	14.621171	-0.055276	4.637194
267.308847	7393.211450	14.626176	-0.055273	4.634756
267.577356	7385.202290	14.631181	-0.055318	4.632323
267.406709	7377.116495	14.636186	-0.055281	4.629867
267.224052	7369.198295	14.641191	-0.055243	4.627460
267.086509	7361.130417	14.646195	-0.055212	4.625006
267.359801	7353.229271	14.651200	-0.055258	4.622601
267.043335	7345.165698	14.656205	-0.055194	4.620146
266.939458	7337.172206	14.661210	-0.055170	4.617711
267.050356	7329.163578	14.666215	-0.055185	4.615270
266.975541	7321.153000	14.671219	-0.055166	4.612827
266.895268	7313.167161	14.676224	-0.055147	4.610390
266.895340	7305.168177	14.681229	-0.055142	4.607948
266.761597	7297.189860	14.686234	-0.055112	4.605511
267.043117	7289.198168	14.691239	-0.055159	4.603069
266.725473	7281.164206	14.696243	-0.055095	4.600612
266.758701	7273.183249	14.701248	-0.055096	4.598170
266.642223	7265.159817	14.706253	-0.055070	4.595714
266.572929	7257.143715	14.711258	-0.055052	4.593259
266.648087	7249.099097	14.716263	-0.055061	4.590794
266.484105	7241.099947	14.721267	-0.055025	4.588341
266.460482	7233.096716	14.726272	-0.055016	4.585886
266.413323	7225.126314	14.731277	-0.055002	4.583440
266.419699	7217.122457	14.736282	-0.054999	4.580982
266.329334	7209.160742	14.741287	-0.054977	4.578535
266.230362	7201.105886	14.746291	-0.054953	4.576059
266.416965	7193.129656	14.751296	-0.054983	4.573606
266.200925	7185.101136	14.756301	-0.054938	4.571135
266.157718	7177.101798	14.761306	-0.054925	4.568671
266.220166	7169.125663	14.766311	-0.054932	4.566214
266.054831	7161.093925	14.771315	-0.054896	4.563738
266.087039	7153.149818	14.776320	-0.054897	4.561288
266.136010	7145.147196	14.781325	-0.054901	4.558818
266.205033	7137.148812	14.786330	-0.054909	4.556349
266.268081	7129.128504	14.791335	-0.054916	4.553871
266.009907	7121.064603	14.796339	-0.054863	4.551378
265.946546	7113.090042	14.801344	-0.054846	4.548912
265.860444	7105.085661	14.806349	-0.054825	4.546435
265.888447	7097.078015	14.811354	-0.054825	4.543956
266.112299	7089.155259	14.816359	-0.054862	4.541502
265.965203	7081.084767	14.821363	-0.054830	4.539000
265.880126	7073.154292	14.826368	-0.054809	4.536541
265.861049	7065.117105	14.831373	-0.054800	4.534047
265.962940	7057.099674	14.836378	-0.054814	4.531558
265.606236	7049.057456	14.841383	-0.054743	4.529059
265.543398	7041.083124	14.846387	-0.054726	4.526581
265.649029	7033.127082	14.851392	-0.054741	4.524107
265.591597	7025.172504	14.856397	-0.054725	4.521632
265.620332	7017.120423	14.861402	-0.054726	4.519125
265.892019	7009.124093	14.866407	-0.054771	4.516635
265.491673	7001.073147	14.871411	-0.054692	4.514125
265.339785	6993.016879	14.876416	-0.054659	4.511612
265.265635	6985.003552	14.881421	-0.054640	4.509112
265.466593	6977.042419	14.886426	-0.054672	4.506627
265.209139	6969.042523	14.891431	-0.054619	4.504127
265.079879	6961.078024	14.896435	-0.054590	4.501638
265.234706	6953.048600	14.901440	-0.054614	4.499127
265.128841	6945.091802	14.906445	-0.054590	4.496638
264.997637	6937.038998	14.911450	-0.054560	4.494116
264.972988	6929.059517	14.916455	-0.054551	4.491617
264.937041	6921.006925	14.921459	-0.054539	4.489093
264.808135	6913.076249	14.926464	-0.054510	4.486606
264.945214	6905.034957	14.931469	-0.054531	4.484083
265.000239	6897.076529	14.936474	-0.054536	4.481585
265.032933	6889.076056	14.941479	-0.054537	4.479072
264.807161	6881.051028	14.946483	-0.054490	4.476549
264.975909	6873.056139	14.951488	-0.054517	4.474036
264.693162	6865.022037	14.956493	-0.054459	4.471507
264.617865	6856.969462	14.961498	-0.054440	4.468971
264.854435	6849.035856	14.966503	-0.054479	4.466473
264.726958	6841.018717	14.971507	-0.054450	4.463946
264.577734	6833.069775	14.976512	-0.054418	4.461439
264.464887	6825.056680	14.981517	-0.054392	4.458910
264.587624	6817.026539	14.986522	-0.054410	4.456375
264.573652	6809.072763	14.991527	-0.054402	4.453863
264.466509	6800.979499	14.996531	-0.054377	4.451304
264.418815	6792.989858	15.001536	-0.054363	4.448777
264.292720	6784.996918	15.006541	-0.054335	4.446247
264.328288	6777.013366	15.011546	-0.054336	4.443720
264.231257	6769.062714	15.016551	-0.054314	4.441201
264.168258	6761.006864	15.021555	-0.054297	4.438647
264.143659	6753.027979	15.026560	-0.054287	4.436116
264.207321	6744.974741	15.031565	-0.054294	4.433561
264.140374	6736.924037	15.036570	-0.054277	4.431004
264.038640	6728.969870	15.041575	-0.054253	4.428477
263.926658	6720.919315	15.046579	-0.054227	4.425917
264.011176	6712.977541	15.051584	-0.054238	4.423391
263.762185	6705.006988	15.056589	-0.054186	4.420853
263.546402	6697.002393	15.061594	-0.054141	4.418303
263.667053	6688.976812	15.066599	-0.054159	4.415747
263.703092	6680.956167	15.071603	-0.054161	4.413190
263.535387	6672.950198	15.076608	-0.054124	4.410635
263.464956	6664.966958	15.081613	-0.054106	4.408086
263.435700	6656.978916	15.086618	-0.054096	4.405535
263.265011	6649.017347	15.091623	-0.054059	4.402990
263.202563	6640.968877	15.096627	-0.054043	4.400416
263.438326	6633.004095	15.101632	-0.054082	4.397869
263.408827	6624.987846	15.106637	-0.054071	4.395303
263.124535	6616.975757	15.111642	-0.054013	4.392735
263.376902	6608.937826	15.116647	-0.054055	4.390161
263.079705	6600.945213	15.121651	-0.053995	4.387596
263.132784	6592.951243	15.126656	-0.054000	4.385031
263.147250	6584.971372	15.131661	-0.053998	4.382469
263.088273	6576.934337	15.136666	-0.053982	4.379887
263.093566	6569.015482	15.141671	-0.053978	4.377342
262.975176	6560.961827	15.146675	-0.053951	4.374751
262.833836	6552.983252	15.151680	-0.053919	4.372182
262.731136	6544.945703	15.156685	-0.053895	4.369593
262.888466	6536.971976	15.161690	-0.053920	4.367025
262.723999	6528.961601	15.166695	-0.053884	4.364442
262.677489	6521.007946	15.171699	-0.053871	4.361876
262.726098	6512.996222	15.176704	-0.053875	4.359290
262.791741	6505.043022	15.181709	-0.053882	4.356722
262.560559	6496.916895	15.186714	-0.053834	4.354095
262.743280	6488.882048	15.191719	-0.053863	4.351498
262.618457	6480.885182	15.196723	-0.053835	4.348910
262.326800	6472.926436	15.201728	-0.053775	4.346331
262.537303	6464.955412	15.206733	-0.053810	4.343750
262.380964	6456.965889	15.211738	-0.053776	4.341160
262.247044	6448.955711	15.216743	-0.053746	4.338561
262.307139	6440.918380	15.221747	-0.053752	4.335953
262.282255	6432.968429	15.226752	-0.053742	4.333372
262.159839	6424.927362	15.231757	-0.053715	4.330758
262.185235	6416.893738	15.236762	-0.053714	4.328147
262.087487	6408.990482	15.241767	-0.053691	4.325575
262.014962	6400.924568	15.246771	-0.053673	4.322949
262.186897	6392.947232	15.251776	-0.053700	4.320352
262.007957	6384.970113	15.256781	-0.053662	4.317751
261.912817	6376.943328	15.261786	-0.053639	4.315133
261.898847	6368.929158	15.266791	-0.053631	4.312518
261.797931	6360.897980	15.271795	-0.053608	4.309895
262.167053	6352.893230	15.276800	-0.053671	4.307283
261.922486	6344.908619	15.281805	-0.053621	4.304671
261.894959	6336.942885	15.286810	-0.053611	4.302066
261.926669	6328.916682	15.291815	-0.053612	4.299439
261.671031	6320.981423	15.296819	-0.053559	4.296839
261.566192	6312.911203	15.301824	-0.053535	4.294193
261.594029	6304.883679	15.306829	-0.053535	4.291561
261.500915	6296.876436	15.311834	-0.053513	4.288934
261.494451	6288.903357	15.316839	-0.053506	4.286316
261.288985	6280.907855	15.321843	-0.053463	4.283688
261.658512	6272.929377	15.326848	-0.053527	4.281069
261.371940	6264.940116	15.331853	-0.053469	4.278439
261.467624	6256.959340	15.336858	-0.053482	4.275813
261.404004	6248.893731	15.341863	-0.053465	4.273157
261.202562	6240.833925	15.346867	-0.053422	4.270499
261.179957	6232.854038	15.351872	-0.053413	4.267868
261.201496	6224.896840	15.356877	-0.053412	4.265243
261.071516	6216.913600	15.361882	-0.053383	4.262606
261.217222	6208.870316	15.366887	-0.053405	4.259951
261.042410	6200.903935	15.371891	-0.053368	4.257316
261.139125	6192.890810	15.376896	-0.053381	4.254667
260.812608	6184.914067	15.381901	-0.053315	4.252024
260.506088	6176.823118	15.386906	-0.053253	4.249342
260.538726	6168.913517	15.391911	-0.053254	4.246721
260.475755	6160.872160	15.396915	-0.053237	4.244055
260.530154	6152.980268	15.401920	-0.053243	4.241437
260.503086	6144.950770	15.406925	-0.053233	4.238771
260.309120	6136.940512	15.411930	-0.053192	4.236108
260.386401	6128.933197	15.416935	-0.053201	4.233447
260.478049	6120.870421	15.421939	-0.053213	4.230766
260.481742	6112.907193	15.426944	-0.053209	4.228116
260.402953	6104.879226	15.431949	-0.053189	4.225442
260.379780	6096.896881	15.436954	-0.053180	4.222782
260.489839	6088.903448	15.441959	-0.053196	4.220117
260.403323	6080.942430	15.446963	-0.053174	4.217460
260.197588	6072.933980	15.451968	-0.053131	4.214784
260.199330	6064.936554	15.456973	-0.053127	4.212112
260.073075	6056.862228	15.461978	-0.053098	4.209412
259.928843	6048.969097	15.466983	-0.053066	4.206770
259.877539	6040.932661	15.471987	-0.053052	4.204079
260.006299	6032.955427	15.476992	-0.053071	4.201409
259.970691	6024.963225	15.481997	-0.053059	4.198730
259.817718	6016.887715	15.487002	-0.053026	4.196020
259.850976	6008.875757	15.492007	-0.053027	4.193332
259.667883	6000.812633	15.497011	-0.052988	4.190622
259.621778	5992.847933	15.502016	-0.052974	4.187945
259.622038	5984.884998	15.507021	-0.052970	4.185268
259.744956	5976.892569	15.512026	-0.052987	4.182580
259.686050	5968.910249	15.517031	-0.052972	4.179892
259.583970	5960.897458	15.522035	-0.052948	4.177192
259.474269	5952.876262	15.527040	-0.052922	4.174486
259.473701	5944.902949	15.532045	-0.052917	4.171797
259.467477	5936.846211	15.537050	-0.052911	4.169077
259.357010	5928.901737	15.542055	-0.052885	4.166393
259.337905	5920.917789	15.547059	-0.052877	4.163694
259.320395	5912.867000	15.552064	-0.052869	4.160971
259.355622	5904.913754	15.557069	-0.052870	4.158280
259.245591	5896.882176	15.562074	-0.052845	4.155559
259.424303	5888.877229	15.567079	-0.052873	4.152848
259.282356	5880.870197	15.572083	-0.052842	4.150131
259.257628	5872.868049	15.577088	-0.052832	4.147416
259.327739	5864.865982	15.582093	-0.052840	4.144700
259.120813	5856.905583	15.587098	-0.052797	4.141993
259.151065	5848.891551	15.592103	-0.052798	4.139268
259.063838	5840.894332	15.597107	-0.052776	4.136547
258.967753	5832.867901	15.602112	-0.052754	4.133813
258.966167	5824.878222	15.607117	-0.052748	4.131091
258.993698	5816.833246	15.612122	-0.052748	4.128349
258.961573	5808.879052	15.617127	-0.052738	4.125635
258.893494	5800.904916	15.622131	-0.052720	4.122913
258.803316	5792.874766	15.627136	-0.052698	4.120169
258.801122	5784.924357	15.632141	-0.052693	4.117451
258.678543	5776.892446	15.637146	-0.052665	4.114703
258.472465	5768.854503	15.642151	-0.052622	4.111949
258.388054	5760.831117	15.647155	-0.052601	4.109200
258.357248	5752.836608	15.652160	-0.052590	4.106460
258.375456	5744.835577	15.657165	-0.052589	4.103716
258.347105	5736.850773	15.662170	-0.052578	4.100976
258.607582	5728.868388	15.667175	-0.052622	4.098238
258.162092	5720.901289	15.672179	-0.052534	4.095495
258.311793	5712.906596	15.677184	-0.052557	4.092748
258.364347	5704.875661	15.682189	-0.052562	4.089985
258.131593	5696.899409	15.687194	-0.052514	4.087235
258.163712	5688.891002	15.692199	-0.052515	4.084476
258.028344	5680.942614	15.697203	-0.052484	4.081734
258.002732	5672.923798	15.702208	-0.052475	4.078967
258.079440	5664.960581	15.707213	-0.052484	4.076219
257.993369	5656.864725	15.712218	-0.052463	4.073421
257.876174	5648.903917	15.717223	-0.052436	4.070667
257.633252	5640.898632	15.722227	-0.052386	4.067894
257.754474	5632.889459	15.727232	-0.052404	4.065123
257.851772	5624.941638	15.732237	-0.052417	4.062371
257.628218	5616.904359	15.737242	-0.052370	4.059581
257.655902	5608.950467	15.742247	-0.052371	4.056822
257.553155	5600.940878	15.747251	-0.052346	4.054040
257.617802	5592.905587	15.752256	-0.052354	4.051250
257.451942	5584.911523	15.757261	-0.052318	4.048468
257.370606	5576.885372	15.762266	-0.052298	4.045675
257.371162	5568.950092	15.767271	-0.052293	4.042913
257.384848	5560.930988	15.772275	-0.052290	4.040119
257.233534	5552.957610	15.777280	-0.052257	4.037338
257.384130	5544.932099	15.782285	-0.052280	4.034540
257.101028	5536.789547	15.787290	-0.052223	4.031694
257.152353	5528.840292	15.792295	-0.052227	4.028918
257.106725	5520.873936	15.797299	-0.052214	4.026132
257.077194	5512.904385	15.802304	-0.052203	4.023344
257.022795	5504.928989	15.807309	-0.052188	4.020551
256.998294	5496.907061	15.812314	-0.052179	4.017741
256.858039	5488.903013	15.817319	-0.052148	4.014933
256.903076	5480.886600	15.822323	-0.052151	4.012122
256.895167	5472.862156	15.827328	-0.052145	4.009305
256.784241	5464.906622	15.832333	-0.052119	4.006508
256.758138	5456.893389	15.837338	-0.052109	4.003691
256.830375	5448.912413	15.842343	-0.052118	4.000885
256.656230	5440.912751	15.847347	-0.052080	3.998066
256.773140	5432.908182	15.852352	-0.052097	3.995248
256.696063	5424.892437	15.857357	-0.052078	3.992421
256.399666	5416.850928	15.862362	-0.052018	3.989579
256.541947	5408.917877	15.867367	-0.052039	3.986781
256.516577	5400.897418	15.872371	-0.052030	3.983947
256.458246	5392.930124	15.877376	-0.052014	3.981129
256.307793	5384.942820	15.882381	-0.051981	3.978301
256.150049	5376.913126	15.887386	-0.051946	3.975456
256.301517	5368.900204	15.892391	-0.051970	3.972620
256.384224	5360.906769	15.897395	-0.051980	3.969787
256.358290	5352.927700	15.902400	-0.051970	3.966956
256.209901	5344.919762	15.907405	-0.051938	3.964110
256.167743	5336.957343	15.912410	-0.051925	3.961280
256.253096	5328.956754	15.917415	-0.051936	3.958437
256.107910	5320.961630	15.922419	-0.051904	3.955590
255.997563	5312.923310	15.927424	-0.051878	3.952725
255.924839	5304.936330	15.932429	-0.051860	3.949878
255.896756	5296.942459	15.937434	-0.051850	3.947027
255.836180	5288.942860	15.942439	-0.051833	3.944172
255.830030	5280.984855	15.947443	-0.051827	3.941330
255.563434	5272.969520	15.952448	-0.051773	3.938460
255.449348	5264.996196	15.957453	-0.051747	3.935607
255.534475	5256.940284	15.962458	-0.051757	3.932725
255.554965	5248.930956	15.967463	-0.051756	3.929857
255.411430	5240.958362	15.972467	-0.051725	3.926997
255.397955	5232.922429	15.977472	-0.051717	3.924115
255.562415	5225.022508	15.982477	-0.051743	3.921282
255.309808	5217.014782	15.987482	-0.051691	3.918401
255.376315	5208.994157	15.992487	-0.051698	3.915519
255.172307	5200.963788	15.997491	-0.051655	3.912626
255.263104	5192.934682	16.002496	-0.051667	3.909738
255.130522	5184.968928	16.007501	-0.051638	3.906865
255.059942	5176.960867	16.012506	-0.051620	3.903977
255.369545	5168.984829	16.017511	-0.051672	3.901105
255.286360	5160.992703	16.022515	-0.051652	3.898218
255.031929	5152.989607	16.027520	-0.051600	3.895321
255.183382	5144.966042	16.032525	-0.051623	3.892423
254.895994	5136.962949	16.037530	-0.051564	3.889521
254.795701	5129.000850	16.042535	-0.051541	3.886636
254.840048	5120.956934	16.047539	-0.051544	3.883721
254.788676	5112.977504	16.052544	-0.051529	3.880826
254.731351	5105.014692	16.057549	-0.051514	3.877935
254.729752	5096.976668	16.062554	-0.051509	3.875015
254.717105	5088.764158	16.067559	-0.051501	3.872030
254.612999	5080.768834	16.072563	-0.051477	3.869119
254.492108	5072.853353	16.077568	-0.051449	3.866235
254.607668	5064.927509	16.082573	-0.051466	3.863350
254.461401	5056.934574	16.087578	-0.051434	3.860433
254.375706	5048.970934	16.092583	-0.051413	3.857525
254.341355	5040.948977	16.097587	-0.051402	3.854595
254.399140	5032.920356	16.102592	-0.051407	3.851662
254.390938	5024.942456	16.107597	-0.051401	3.848744
254.208304	5016.950490	16.112602	-0.051362	3.845816
254.205052	5008.987896	16.117607	-0.051356	3.842899
254.114869	5001.011542	16.122611	-0.051335	3.839973
253.968689	4993.046166	16.127616	-0.051302	3.837048
253.895620	4985.023297	16.132621	-0.051284	3.834102
253.768695	4977.005439	16.137626	-0.051255	3.831153
253.933585	4968.997587	16.142631	-0.051281	3.828212
253.695648	4961.005244	16.147635	-0.051232	3.825266
253.874457	4953.024961	16.152640	-0.051260	3.822331
253.896890	4945.036859	16.157645	-0.051259	3.819388
253.686483	4937.105565	16.162650	-0.051215	3.816458
253.842170	4929.047676	16.167655	-0.051239	3.813487
253.987084	4921.058304	16.172659	-0.051261	3.810539
253.580396	4913.045553	16.177664	-0.051181	3.807568
253.492413	4905.069542	16.182669	-0.051159	3.804615
253.604905	4897.069472	16.187674	-0.051175	3.801656
253.535265	4889.099776	16.192679	-0.051157	3.798701
253.301407	4881.109820	16.197683	-0.051109	3.795733
253.318787	4873.045760	16.202688	-0.051107	3.792741
253.274818	4865.032036	16.207693	-0.051094	3.789763
253.228422	4857.030657	16.212698	-0.051080	3.786788
253.288810	4849.051859	16.217703	-0.051087	3.783821
253.236675	4841.088561	16.222707	-0.051072	3.780855
253.024919	4833.085865	16.227712	-0.051028	3.777869
253.122862	4825.096008	16.232717	-0.051041	3.774892
252.913092	4817.064989	16.237722	-0.050997	3.771890
252.943743	4809.056770	16.242727	-0.050998	3.768899
252.811823	4801.081506	16.247731	-0.050968	3.765915
252.813940	4793.081906	16.252736	-0.050964	3.762923
252.950385	4785.117115	16.257741	-0.050984	3.759944
252.731017	4777.118836	16.262746	-0.050938	3.756942
252.633489	4769.100390	16.267751	-0.050915	3.753934
252.877508	4761.052308	16.272755	-0.050956	3.750919
252.746682	4753.056309	16.277760	-0.050926	3.747913
252.878966	4745.105194	16.282765	-0.050946	3.744927
252.758100	4737.100694	16.287770	-0.050919	3.741913
252.445265	4729.122196	16.292775	-0.050855	3.738902
252.636565	4721.106146	16.297779	-0.050886	3.735886
252.554773	4713.083096	16.302784	-0.050866	3.732859
252.694712	4705.093085	16.307789	-0.050887	3.729847
252.205388	4697.119661	16.312794	-0.050791	3.726823
252.374453	4689.139089	16.317799	-0.050817	3.723811
252.382381	4681.208189	16.322803	-0.050814	3.720810
252.217258	4673.205756	16.327808	-0.050778	3.717776
252.171261	4665.180046	16.332813	-0.050765	3.714734
252.067447	4657.079086	16.337818	-0.050740	3.711659
252.171078	4649.095633	16.342823	-0.050755	3.708631
252.127900	4641.080528	16.347827	-0.050742	3.705586
251.835499	4633.139950	16.352832	-0.050682	3.702559
251.908233	4625.166608	16.357837	-0.050691	3.699527
251.814412	4617.174611	16.362842	-0.050669	3.696481
251.883503	4609.179383	16.367847	-0.050676	3.693436
251.761457	4601.167300	16.372851	-0.050649	3.690377
251.671024	4593.187627	16.377856	-0.050627	3.687328
251.754171	4585.188413	16.382861	-0.050638	3.684274
251.648700	4577.216478	16.387866	-0.050613	3.681223
251.914162	4569.194717	16.392871	-0.050657	3.678159
251.601983	4561.238450	16.397875	-0.050594	3.675104
251.515280	4553.211169	16.402880	-0.050573	3.672024
251.712930	4545.207365	16.407885	-0.050605	3.668959
251.596165	4537.176075	16.412890	-0.050578	3.665871
251.558166	4529.230736	16.417895	-0.050566	3.662817
251.600075	4521.209562	16.422899	-0.050569	3.659733
251.600026	4513.245002	16.427904	-0.050564	3.656667
251.565515	4505.261126	16.432909	-0.050553	3.653590
251.300253	4497.216402	16.437914	-0.050498	3.650480
251.271958	4489.252986	16.442919	-0.050488	3.647406
251.049361	4481.219164	16.447923	-0.050442	3.644297
250.901789	4473.262204	16.452928	-0.050409	3.641217
251.210371	4465.270865	16.457933	-0.050462	3.638133
251.034956	4457.267313	16.462938	-0.050424	3.635029
250.879491	4449.245142	16.467943	-0.050390	3.631915
250.894256	4441.217265	16.472947	-0.050388	3.628801
250.956373	4433.223513	16.477952	-0.050395	3.625699
250.749655	4425.285922	16.482957	-0.050351	3.622609
250.614563	4417.251482	16.487962	-0.050321	3.619480
250.730038	4409.327460	16.492967	-0.050338	3.616399
250.671783	4401.293456	16.497971	-0.050322	3.613267
250.669900	4393.261656	16.502976	-0.050317	3.610135
250.827907	4385.296644	16.507981	-0.050341	3.607031
250.667836	4377.280379	16.512986	-0.050306	3.603895
250.384659	4369.339023	16.517991	-0.050249	3.600783
250.423434	4361.360088	16.522995	-0.050251	3.597662
250.335592	4353.366076	16.528000	-0.050230	3.594528
250.352407	4345.358810	16.533005	-0.050228	3.591390
250.343717	4337.318224	16.538010	-0.050221	3.588235
250.438877	4329.337602	16.543015	-0.050234	3.585104
250.266343	4321.386511	16.548019	-0.050197	3.581975
250.093527	4313.381388	16.553024	-0.050160	3.578821
250.146455	4305.408155	16.558029	-0.050165	3.575683
250.281455	4297.347205	16.563034	-0.050185	3.572510
250.028372	4289.355837	16.568039	-0.050133	3.569351
250.179503	4281.409142	16.573043	-0.050156	3.566219
250.086373	4273.421814	16.578048	-0.050134	3.563060
250.144480	4265.420971	16.583053	-0.050140	3.559898
249.952309	4257.429202	16.588058	-0.050099	3.556729
250.081384	4249.369583	16.593063	-0.050118	3.553540
249.935145	4241.338439	16.598067	-0.050086	3.550351
249.666462	4233.350459	16.603072	-0.050031	3.547173
249.722792	4225.378425	16.608077	-0.050036	3.544008
249.689349	4217.403748	16.613082	-0.050025	3.540836
249.676830	4209.401727	16.618087	-0.050018	3.537651
249.435089	4201.425784	16.623091	-0.049968	3.534467
249.484397	4193.401469	16.628096	-0.049972	3.531270
249.458698	4185.429977	16.633101	-0.049962	3.528088
249.256868	4177.413452	16.638106	-0.049920	3.524880
249.432431	4169.432540	16.643111	-0.049948	3.521695
249.570450	4161.452284	16.648115	-0.049968	3.518506
249.277495	4153.482610	16.653120	-0.049909	3.515306
249.486387	4145.463107	16.658125	-0.049943	3.512098
249.216924	4137.443339	16.663130	-0.049888	3.508872
249.004577	4129.474843	16.668135	-0.049843	3.505665
249.026054	4121.520488	16.673139	-0.049842	3.502468
249.078655	4113.468593	16.678144	-0.049847	3.499231
249.319749	4105.522610	16.683149	-0.049887	3.496038
249.079479	4097.522982	16.688154	-0.049837	3.492806
248.943932	4089.498710	16.693159	-0.049807	3.489565
249.025870	4081.530607	16.698163	-0.049818	3.486350
248.677581	4073.561922	16.703168	-0.049748	3.483118
248.607140	4065.588947	16.708173	-0.049730	3.479890
248.802786	4057.618588	16.713178	-0.049761	3.476669
248.736236	4049.566952	16.718183	-0.049744	3.473403
248.753311	4041.537827	16.723187	-0.049742	3.470146
248.577888	4033.551522	16.728192	-0.049704	3.466897
248.808243	4025.574993	16.733197	-0.049742	3.463663
248.483256	4017.550474	16.738202	-0.049677	3.460387
248.539285	4009.619665	16.743207	-0.049682	3.457160
248.475937	4001.618552	16.748211	-0.049666	3.453896
248.395748	3993.578971	16.753216	-0.049646	3.450613
248.380282	3985.640430	16.758221	-0.049638	3.447371
248.266786	3977.595919	16.763226	-0.049612	3.444079
248.048087	3969.668354	16.768231	-0.049566	3.440828
248.061968	3961.668535	16.773235	-0.049564	3.437552
248.175656	3953.626347	16.778240	-0.049580	3.434259
248.255755	3945.644756	16.783245	-0.049590	3.430986
247.971796	3937.657234	16.788250	-0.049532	3.427696
247.980481	3929.629984	16.793255	-0.049529	3.424396
248.119016	3921.689273	16.798259	-0.049550	3.421133
247.963765	3913.665899	16.803264	-0.049516	3.417823
247.809762	3905.719898	16.808269	-0.049482	3.414541
247.855958	3897.693965	16.813274	-0.049486	3.411230
247.775049	3889.687866	16.818279	-0.049466	3.407920
247.590779	3881.729124	16.823283	-0.049427	3.404623
247.402161	3873.762714	16.828288	-0.049386	3.401319
247.651958	3865.770512	16.833293	-0.049428	3.398016
247.498614	3857.770829	16.838298	-0.049395	3.394693
247.502148	3849.673433	16.843303	-0.049390	3.391331
247.420139	3841.719670	16.848307	-0.049370	3.388023
247.473780	3833.677507	16.853312	-0.049375	3.384680
247.356547	3825.779871	16.858317	-0.049348	3.381387
247.212025	3817.767266	16.863322	-0.049316	3.378043
247.379606	3809.761595	16.868327	-0.049343	3.374709
247.210486	3801.793165	16.873331	-0.049306	3.371375
246.999532	3793.801186	16.878336	-0.049262	3.368027
247.100712	3785.814432	16.883341	-0.049276	3.364688
247.192030	3777.838641	16.888346	-0.049288	3.361351
246.993136	3769.866633	16.893351	-0.049246	3.358001
246.958929	3761.870656	16.898355	-0.049235	3.354644
246.726922	3753.823266	16.903360	-0.049186	3.351255
246.924681	3745.825620	16.908365	-0.049218	3.347899
247.072812	3737.823157	16.913370	-0.049241	3.344536
247.033082	3729.870912	16.918375	-0.049229	3.341183
246.826272	3721.907184	16.923379	-0.049185	3.337816
246.740489	3713.871569	16.928384	-0.049164	3.334420
246.890653	3705.887045	16.933389	-0.049187	3.331051
246.677189	3697.923220	16.938394	-0.049143	3.327674
246.656137	3689.911640	16.943399	-0.049134	3.324280
246.729827	3681.964685	16.948403	-0.049143	3.320913
246.577475	3673.973640	16.953408	-0.049109	3.317516
246.544256	3665.995015	16.958413	-0.049098	3.314125
246.249343	3657.963379	16.963418	-0.049038	3.310699
246.241921	3649.957191	16.968423	-0.049032	3.307290
246.129394	3641.987653	16.973427	-0.049006	3.303890
245.995767	3633.983641	16.978432	-0.048976	3.300470
246.322284	3626.017747	16.983437	-0.049032	3.297081
246.136093	3618.024055	16.988442	-0.048992	3.293657
245.817753	3610.024380	16.993447	-0.048928	3.290221
246.077441	3602.027842	16.998451	-0.048972	3.286806
246.009053	3594.029775	17.003456	-0.048954	3.283373
246.101509	3586.035754	17.008461	-0.048966	3.279945
245.958982	3578.111986	17.013466	-0.048935	3.276535
245.870262	3570.099534	17.018471	-0.048913	3.273085
245.881998	3562.076299	17.023475	-0.048910	3.269630
245.797185	3554.092777	17.028480	-0.048890	3.266185
245.866016	3546.104417	17.033485	-0.048898	3.262741
245.658290	3538.110761	17.038490	-0.048854	3.259280
245.446692	3530.167904	17.043495	-0.048810	3.255836
245.537159	3522.143094	17.048499	-0.048821	3.252366
245.576493	3514.086878	17.053504	-0.048824	3.248876
245.454531	3506.155594	17.058509	-0.048796	3.245430
245.428986	3498.185084	17.063514	-0.048786	3.241968
245.393465	3490.190298	17.068519	-0.048775	3.238491
245.386173	3482.214402	17.073523	-0.048769	3.235019
245.147709	3474.170471	17.078528	-0.048719	3.231504
245.418048	3466.147348	17.083533	-0.048765	3.228016
245.092530	3458.184864	17.088538	-0.048699	3.224526
245.113712	3450.217265	17.093543	-0.048698	3.221044
245.186839	3442.229157	17.098547	-0.048707	3.217551
244.902560	3434.243401	17.103552	-0.048649	3.214041
244.719830	3426.256234	17.108557	-0.048610	3.210531
244.611665	3418.268013	17.113562	-0.048585	3.207019
244.667878	3410.284409	17.118567	-0.048590	3.203513
244.497361	3402.340938	17.123571	-0.048554	3.200010
244.357562	3394.363664	17.128576	-0.048523	3.196491
244.580648	3386.323213	17.133581	-0.048559	3.192954
244.300950	3378.331026	17.138586	-0.048502	3.189414
244.225404	3370.349526	17.143591	-0.048483	3.185884
244.406914	3362.338902	17.148595	-0.048512	3.182347
244.338717	3354.361052	17.153600	-0.048494	3.178810
244.383424	3346.393930	17.158605	-0.048498	3.175279
244.378225	3338.358925	17.163610	-0.048492	3.171712
244.405515	3330.367741	17.168615	-0.048492	3.168162
244.487338	3322.394957	17.173619	-0.048502	3.164618
244.251141	3314.444369	17.178624	-0.048453	3.161066
244.327424	3306.475295	17.183629	-0.048463	3.157516
244.226461	3298.457609	17.188634	-0.048439	3.153932
244.048378	3290.445436	17.193639	-0.048401	3.150344
243.977987	3282.473107	17.198643	-0.048383	3.146773
244.052259	3274.457396	17.203648	-0.048392	3.143186
243.943532	3266.502142	17.208653	-0.048366	3.139613
243.869736	3258.537279	17.213658	-0.048348	3.136034
244.066785	3250.518095	17.218663	-0.048379	3.132438
244.005339	3242.542534	17.223667	-0.048363	3.128846
243.632386	3234.584791	17.228672	-0.048289	3.125244
243.726555	3226.602604	17.233677	-0.048301	3.121648
243.644743	3218.607647	17.238682	-0.048281	3.118034
243.577185	3210.634389	17.243687	-0.048264	3.114426
243.568303	3202.625958	17.248691	-0.048257	3.110801
243.458029	3194.626661	17.253696	-0.048231	3.107171
243.373264	3186.629404	17.258701	-0.048211	3.103539
243.226611	3178.671796	17.263706	-0.048178	3.099918
243.309718	3170.691580	17.268711	-0.048189	3.096292
243.332620	3162.689033	17.273715	-0.048188	3.092650
243.033045	3154.687330	17.278720	-0.048128	3.088989
243.078079	3146.709016	17.283725	-0.048131	3.085350
242.969689	3138.762442	17.288730	-0.048106	3.081714
242.917809	3130.771149	17.293735	-0.048091	3.078056
243.005219	3122.788866	17.298739	-0.048103	3.074404
242.969369	3114.671385	17.303744	-0.048091	3.070680
242.763048	3106.725222	17.308749	-0.048048	3.067022
242.745575	3098.768680	17.313754	-0.048039	3.063364
242.802992	3090.778058	17.318759	-0.048045	3.059690
242.769470	3082.833416	17.323763	-0.048034	3.056028
242.670218	3074.821198	17.328768	-0.048011	3.052327
242.790925	3066.831921	17.333773	-0.048028	3.048642
242.862699	3058.833671	17.338778	-0.048036	3.044947
242.494906	3050.928229	17.343783	-0.047963	3.041270
242.432285	3042.951829	17.348787	-0.047947	3.037569
242.442846	3034.919783	17.353792	-0.047943	3.033842
242.656869	3026.901315	17.358797	-0.047978	3.030126
242.511389	3018.938028	17.363802	-0.047946	3.026414
242.337952	3010.968077	17.368807	-0.047909	3.022693
242.560111	3002.975415	17.373811	-0.047946	3.018976
242.196239	2995.027740	17.378816	-0.047873	3.015246
242.201016	2987.016746	17.383821	-0.047869	3.011501
242.201164	2979.018202	17.388826	-0.047864	3.007756
241.989064	2971.046625	17.393831	-0.047819	3.004009
241.911412	2963.105503	17.398835	-0.047800	3.000279
242.004915	2955.111741	17.403840	-0.047813	2.996527
242.023084	2947.106735	17.408845	-0.047811	2.992761
241.896583	2939.102623	17.413850	-0.047782	2.988984
241.994948	2931.082174	17.418855	-0.047796	2.985206
242.009723	2923.148763	17.423859	-0.047794	2.981460
241.660118	2915.181671	17.428864	-0.047724	2.977675
241.701009	2907.204292	17.433869	-0.047726	2.973900
241.634129	2899.194584	17.438874	-0.047709	2.970099
241.538546	2891.212042	17.443879	-0.047686	2.966305
241.484312	2883.264208	17.448883	-0.047671	2.962525
241.386573	2875.253869	17.453888	-0.047648	2.958707
241.232596	2867.322829	17.458893	-0.047614	2.954920
241.319591	2859.272070	17.463898	-0.047626	2.951083
241.317707	2851.292933	17.468903	-0.047620	2.947271
241.235632	2843.328240	17.473907	-0.047600	2.943456
240.942540	2835.345354	17.478912	-0.047541	2.939617
241.045941	2827.382647	17.483917	-0.047555	2.935803
241.068543	2819.368872	17.488922	-0.047554	2.931956
241.025470	2811.376010	17.493927	-0.047541	2.928110
241.027409	2803.404953	17.498931	-0.047537	2.924272
240.933502	2795.452263	17.503936	-0.047514	2.920432
241.073138	2787.474134	17.508941	-0.047535	2.916588
241.138296	2779.427509	17.513946	-0.047542	2.912701
240.917659	2771.402411	17.518951	-0.047496	2.908805
240.809964	2763.459407	17.523955	-0.047471	2.904949
240.762044	2755.496624	17.528960	-0.047457	2.901081
240.660100	2747.557521	17.533965	-0.047434	2.897217
240.678791	2739.560567	17.538970	-0.047432	2.893326
240.560579	2731.546023	17.543975	-0.047405	2.889414
240.506797	2723.596607	17.548979	-0.047390	2.885532
240.265521	2715.644964	17.553984	-0.047340	2.881633
240.380176	2707.655571	17.558989	-0.047357	2.877730
240.387992	2699.659609	17.563994	-0.047353	2.873812
240.390175	2691.626215	17.568999	-0.047349	2.869871
240.359000	2683.699668	17.574003	-0.047338	2.865974
240.246033	2675.698623	17.579008	-0.047312	2.862032
240.054228	2667.766929	17.584013	-0.047271	2.858113
240.209320	2659.766637	17.589018	-0.047295	2.854175
240.077387	2651.772458	17.594023	-0.047266	2.850218
239.932478	2643.825602	17.599027	-0.047234	2.846278
239.891856	2635.828891	17.604032	-0.047221	2.842314
239.902532	2627.868977	17.609037	-0.047218	2.838366
239.897840	2619.891108	17.614042	-0.047213	2.834402
239.752616	2611.854496	17.619047	-0.047181	2.830396
239.915741	2603.879326	17.624051	-0.047206	2.826432
239.662922	2595.932146	17.629056	-0.047154	2.822452
239.401546	2587.982304	17.634061	-0.047100	2.818466
239.345178	2579.992910	17.639066	-0.047085	2.814465
239.583577	2571.941201	17.644071	-0.047124	2.810445
239.450448	2564.012017	17.649075	-0.047095	2.806458
239.099128	2556.070887	17.654080	-0.047024	2.802448
239.353465	2548.076363	17.659085	-0.047067	2.798440
239.276155	2540.104877	17.664090	-0.047047	2.794418
238.965375	2532.108274	17.669095	-0.046985	2.790365
239.285773	2524.109497	17.674099	-0.047039	2.786341
239.184999	2516.142683	17.679104	-0.047016	2.782303
239.170437	2508.185455	17.684109	-0.047008	2.778269
238.851399	2500.242715	17.689114	-0.046944	2.774219
238.812337	2492.226890	17.694119	-0.046931	2.770142
239.061262	2484.229029	17.699123	-0.046973	2.766085
238.864033	2476.275455	17.704128	-0.046931	2.762018
238.923947	2468.312078	17.709133	-0.046937	2.757956
238.787314	2460.321275	17.714138	-0.046907	2.753862
238.666459	2452.260769	17.719143	-0.046879	2.749727
238.750008	2444.319122	17.724147	-0.046890	2.745659
238.596670	2436.362518	17.729152	-0.046857	2.741563
238.475727	2428.409810	17.734157	-0.046829	2.737464
238.259705	2420.458547	17.739162	-0.046784	2.733355
238.341613	2412.424135	17.744167	-0.046794	2.729214
238.226020	2404.499606	17.749171	-0.046768	2.725112
238.084642	2396.524438	17.754176	-0.046737	2.720976
238.066055	2388.579326	17.759181	-0.046728	2.716857
237.990060	2380.584022	17.764186	-0.046709	2.712702
238.149842	2372.538588	17.769191	-0.046734	2.708529
238.155479	2364.603618	17.774195	-0.046730	2.704398
238.143086	2356.625505	17.779200	-0.046723	2.700237
238.081629	2348.690681	17.784205	-0.046706	2.696088
237.762441	2340.708499	17.789210	-0.046642	2.691893
237.824076	2332.710265	17.794215	-0.046649	2.687706
237.799684	2324.754469	17.799219	-0.046639	2.683530
237.820772	2316.753924	17.804224	-0.046638	2.679326
238.019249	2308.813161	17.809229	-0.046670	2.675159
237.783417	2300.810761	17.814234	-0.046621	2.670925
237.708297	2292.834721	17.819239	-0.046602	2.666708
237.586954	2284.876377	17.824243	-0.046575	2.662492
237.583320	2276.918114	17.829248	-0.046569	2.658276
237.461904	2268.943359	17.834253	-0.046542	2.654037
237.310029	2260.973105	17.839258	-0.046508	2.649791
237.336849	2252.981792	17.844263	-0.046508	2.645539
237.505008	2245.027792	17.849267	-0.046535	2.641310
237.241081	2237.073253	17.854272	-0.046481	2.637045
237.164602	2229.088819	17.859277	-0.046462	2.632769
237.166327	2221.096397	17.864282	-0.046457	2.628488
236.898473	2213.133436	17.869287	-0.046402	2.624197
236.917184	2205.183308	17.874291	-0.046401	2.619925
236.802218	2197.214604	17.879296	-0.046374	2.615627
236.983622	2189.211577	17.884301	-0.046403	2.611324
236.789491	2181.263402	17.889306	-0.046362	2.607018
236.638566	2173.283886	17.894311	-0.046329	2.602690
236.832337	2165.332880	17.899315	-0.046360	2.598394
236.840288	2157.328178	17.904320	-0.046357	2.594049
236.728915	2149.186016	17.909325	-0.046331	2.589615
236.618424	2141.270787	17.914330	-0.046305	2.585296
236.450279	2133.346064	17.919335	-0.046269	2.580960
236.409571	2125.418451	17.924339	-0.046257	2.576625
236.246453	2117.449520	17.929344	-0.046221	2.572251
236.265207	2109.479561	17.934349	-0.046220	2.567882
236.289134	2101.506312	17.939354	-0.046220	2.563504
236.168412	2093.572605	17.944359	-0.046192	2.559130
236.238145	2085.625867	17.949363	-0.046200	2.554755
236.041617	2077.621664	17.954368	-0.046159	2.550321
235.825918	2069.682708	17.959373	-0.046114	2.545915
235.992015	2061.704273	17.964378	-0.046140	2.541506
235.975188	2053.742927	17.969383	-0.046132	2.537086
235.844389	2045.799060	17.974387	-0.046102	2.532660
235.774080	2037.811022	17.979392	-0.046084	2.528206
235.828540	2029.841815	17.984397	-0.046089	2.523764
235.868316	2021.883740	17.989402	-0.046092	2.519318
235.831806	2013.931923	17.994407	-0.046080	2.514863
235.696405	2005.940752	17.999411	-0.046050	2.510371
235.594018	1997.963319	18.004416	-0.046026	2.505881
235.607537	1990.014387	18.009421	-0.046024	2.501407
235.585650	1982.069299	18.014426	-0.046015	2.496925
235.399305	1974.089634	18.019431	-0.045975	2.492403
235.282652	1966.138680	18.024435	-0.045948	2.487894
235.257984	1958.156994	18.029440	-0.045939	2.483366
235.243475	1950.214359	18.034445	-0.045931	2.478853
235.006450	1942.283347	18.039450	-0.045882	2.474322
234.910148	1934.273724	18.044455	-0.045859	2.469748
235.222050	1926.277336	18.049459	-0.045912	2.465204
234.914882	1918.356482	18.054464	-0.045850	2.460648
234.996165	1910.395844	18.059469	-0.045860	2.456090
235.041057	1902.420484	18.064474	-0.045864	2.451512
234.968522	1894.439623	18.069479	-0.045845	2.446914
234.822331	1886.529735	18.074483	-0.045813	2.442343
234.701156	1878.568273	18.079488	-0.045786	2.437735
234.734072	1870.579256	18.084493	-0.045787	2.433114
234.732165	1862.561572	18.089498	-0.045782	2.428464
234.491276	1854.626798	18.094503	-0.045732	2.423836
234.435004	1846.685025	18.099507	-0.045717	2.419209
234.268035	1838.745874	18.104512	-0.045681	2.414566
234.327655	1830.739428	18.109517	-0.045687	2.409893
234.254076	1822.802403	18.114522	-0.045668	2.405240
234.198818	1814.855470	18.119527	-0.045653	2.400574
234.051373	1806.944266	18.124531	-0.045620	2.395913
234.008998	1798.946857	18.129536	-0.045608	2.391200
233.977612	1790.968520	18.134541	-0.045597	2.386490
233.927661	1783.032169	18.139546	-0.045583	2.381795
233.873577	1775.079140	18.144551	-0.045568	2.377079
233.909952	1767.112165	18.149555	-0.045569	2.372353
233.935856	1759.120225	18.154560	-0.045569	2.367602
233.894600	1751.177419	18.159565	-0.045557	2.362865
233.840497	1743.259602	18.164570	-0.045542	2.358133
233.553035	1735.307652	18.169575	-0.045483	2.353352
233.545296	1727.332121	18.174579	-0.045477	2.348569
233.594517	1719.340194	18.179584	-0.045481	2.343772
233.626159	1711.400645	18.184589	-0.045482	2.338995
233.314059	1703.504078	18.189594	-0.045419	2.334206
233.255494	1695.506357	18.194599	-0.045403	2.329366
233.166464	1687.567532	18.199603	-0.045382	2.324550
233.213470	1679.602244	18.204608	-0.045386	2.319719
233.144240	1671.665029	18.209613	-0.045368	2.314885
233.063520	1663.687417	18.214618	-0.045348	2.310015
233.191889	1655.702106	18.219623	-0.045367	2.305148
233.135978	1647.784572	18.224627	-0.045351	2.300297
232.829466	1639.870915	18.229632	-0.045289	2.295417
233.031346	1631.871108	18.234637	-0.045322	2.290516
232.775610	1623.963976	18.239642	-0.045270	2.285623
232.467940	1616.044479	18.244647	-0.045207	2.280707
232.690553	1608.056640	18.249651	-0.045244	2.275784
232.613122	1600.029862	18.254656	-0.045225	2.270800
232.630827	1592.060256	18.259661	-0.045223	2.265849
232.649395	1584.143476	18.264666	-0.045221	2.260921
232.550475	1576.193553	18.269671	-0.045198	2.255950
232.304062	1568.279979	18.274675	-0.045147	2.250978
232.245217	1560.309911	18.279680	-0.045131	2.245977
232.247718	1552.372641	18.284685	-0.045127	2.240990
232.327330	1544.432841	18.289690	-0.045137	2.235997
232.088671	1536.474689	18.294695	-0.045088	2.230953
231.974698	1528.543840	18.299699	-0.045061	2.225926
232.064726	1520.577270	18.304704	-0.045073	2.220883
231.905334	1512.658842	18.309709	-0.045039	2.215837
231.958017	1504.695914	18.314714	-0.045044	2.210771
231.842691	1496.732597	18.319719	-0.045017	2.205677
231.746530	1488.825245	18.324723	-0.044994	2.200609
231.606528	1480.905885	18.329728	-0.044963	2.195517
231.461242	1472.924471	18.334733	-0.044931	2.190373
231.589304	1464.951977	18.339738	-0.044950	2.185248
231.442892	1457.030483	18.344743	-0.044918	2.180119
231.639822	1449.075110	18.349747	-0.044950	2.174987
231.512651	1441.127736	18.354752	-0.044921	2.169818
231.371896	1433.199150	18.359757	-0.044890	2.164648
231.364153	1425.284494	18.364762	-0.044884	2.159487
231.269809	1417.351969	18.369767	-0.044861	2.154293
231.313477	1409.382245	18.374771	-0.044864	2.149076
231.194154	1401.445660	18.379776	-0.044837	2.143852
231.146989	1393.514354	18.384781	-0.044824	2.138626
231.295410	1385.563509	18.389786	-0.044846	2.133393
230.811864	1377.660901	18.394791	-0.044751	2.128119
230.843752	1369.725665	18.399795	-0.044752	2.122859
230.752893	1361.800543	18.404800	-0.044731	2.117581
230.660002	1353.827225	18.409805	-0.044708	2.112257
230.512086	1345.863576	18.414810	-0.044676	2.106921
230.515796	1337.917799	18.419815	-0.044672	2.101598
230.505084	1329.998165	18.424819	-0.044665	2.096278
230.324602	1322.072547	18.429824	-0.044626	2.090924
230.217498	1314.147910	18.434829	-0.044601	2.085563
230.216532	1306.220666	18.439834	-0.044596	2.080198
230.265708	1298.271629	18.444839	-0.044601	2.074809
230.328293	1290.316254	18.449843	-0.044607	2.069402
230.206325	1282.394378	18.454848	-0.044580	2.063986
230.094009	1274.484431	18.459853	-0.044554	2.058565
230.011198	1266.579923	18.464858	-0.044534	2.053137
230.019514	1258.605687	18.469863	-0.044530	2.047655
230.017976	1250.699897	18.474867	-0.044525	2.042204
229.867279	1242.804864	18.479872	-0.044492	2.036732
229.683182	1234.864090	18.484877	-0.044453	2.031209
229.773876	1226.901842	18.489882	-0.044465	2.025685
229.587719	1218.988204	18.494887	-0.044425	2.020150
229.686920	1211.065584	18.499891	-0.044439	2.014624
229.695318	1203.112632	18.504896	-0.044435	2.009052
229.575006	1195.204326	18.509901	-0.044408	2.003482
229.416615	1187.314215	18.514906	-0.044374	1.997906
229.321315	1179.377963	18.519911	-0.044351	1.992288
229.377880	1171.435841	18.524915	-0.044357	1.986666
229.258578	1163.523232	18.529920	-0.044330	1.981030
229.224117	1155.614871	18.534925	-0.044318	1.975390
229.196082	1147.682116	18.539930	-0.044308	1.969718
228.937690	1139.792723	18.544935	-0.044255	1.964035
228.936338	1131.886138	18.549939	-0.044250	1.958351
228.890113	1123.940669	18.554944	-0.044237	1.952618
228.784336	1115.973806	18.559949	-0.044212	1.946845
228.750779	1108.076729	18.564954	-0.044201	1.941114
228.610438	1100.171891	18.569959	-0.044170	1.935349
228.829922	1092.217479	18.574963	-0.044206	1.929570
228.493165	1084.344801	18.579968	-0.044138	1.923772
228.570605	1076.426762	18.584973	-0.044148	1.917969
228.622414	1068.496239	18.589978	-0.044152	1.912136
228.410129	1060.585074	18.594983	-0.044108	1.906271
228.361126	1052.699743	18.599987	-0.044094	1.900424
228.189056	1044.803245	18.604992	-0.044057	1.894537
228.339433	1036.847480	18.609997	-0.044080	1.888625
228.211678	1028.977335	18.615002	-0.044051	1.882726
228.063700	1021.083685	18.620007	-0.044019	1.876788
227.883397	1013.174261	18.625011	-0.043981	1.870816
227.787003	1005.258607	18.630016	-0.043958	1.864830
227.981029	997.324620	18.635021	-0.043989	1.858845
227.895774	989.437408	18.640026	-0.043968	1.852843
227.757490	981.521350	18.645031	-0.043937	1.846793
227.865346	973.618394	18.650035	-0.043953	1.840762
227.702425	965.743002	18.655040	-0.043917	1.834701
227.697645	957.812516	18.660045	-0.043912	1.828596
227.548949	949.944774	18.665050	-0.043879	1.822502
227.337259	942.065495	18.670055	-0.043835	1.816371
227.584232	934.116677	18.675059	-0.043876	1.810220
227.317956	926.256599	18.680064	-0.043821	1.804055
227.099589	918.406414	18.685069	-0.043776	1.797883
227.018133	910.481980	18.690074	-0.043756	1.791648
227.025577	902.532226	18.695079	-0.043752	1.785382
227.078832	894.652647	18.700083	-0.043757	1.779155
226.881431	886.785385	18.705088	-0.043716	1.772885
226.826220	878.884824	18.710093	-0.043701	1.766583
226.810497	871.012337	18.715098	-0.043693	1.760287
226.539820	863.159835	18.720103	-0.043637	1.753952
226.651619	855.230640	18.725107	-0.043653	1.747580
226.555073	847.350870	18.730112	-0.043631	1.741199
226.326647	839.500339	18.735117	-0.043583	1.734801
226.618780	831.567779	18.740122	-0.043633	1.728379
226.462789	823.703320	18.745127	-0.043599	1.721931
226.315667	815.857333	18.750131	-0.043566	1.715476
226.177001	807.968121	18.755136	-0.043536	1.708961
226.118794	800.092613	18.760141	-0.043520	1.702443
226.180811	792.217396	18.765146	-0.043527	1.695916
225.938058	784.343312	18.770151	-0.043477	1.689325
225.920974	776.477653	18.775155	-0.043469	1.682745
225.852750	768.627442	18.780160	-0.043451	1.676145
225.804938	760.731360	18.785165	-0.043437	1.669483
225.870174	752.864474	18.790170	-0.043445	1.662834
225.544695	745.040452	18.795175	-0.043379	1.656142
225.354288	737.195957	18.800179	-0.043339	1.649424
225.436690	729.312245	18.805184	-0.043349	1.642682
225.185316	721.483589	18.810189	-0.043298	1.635913
225.187726	713.557707	18.815194	-0.043293	1.629068
225.102279	705.695284	18.820199	-0.043272	1.622236
225.018085	697.856858	18.825203	-0.043252	1.615397
224.900893	690.007614	18.830208	-0.043225	1.608514
224.714667	682.166045	18.835213	-0.043186	1.601599
224.820402	674.315072	18.840218	-0.043200	1.594687
224.670375	666.460718	18.845223	-0.043168	1.587705
224.549467	658.625108	18.850227	-0.043140	1.580713
224.399233	650.807523	18.855232	-0.043107	1.573702
224.345455	642.946678	18.860237	-0.043093	1.566635
224.313873	635.129088	18.865242	-0.043082	1.559578
224.228485	627.279757	18.870247	-0.043061	1.552452
224.080124	619.435969	18.875251	-0.043029	1.545289
224.157538	611.585190	18.880256	-0.043038	1.538120
223.847487	603.792088	18.885261	-0.042976	1.530913
223.883336	595.953052	18.890266	-0.042977	1.523680
223.965751	588.110620	18.895271	-0.042988	1.516417
224.032214	580.267413	18.900275	-0.042995	1.509116
223.645775	572.502153	18.905280	-0.042919	1.501784
223.402439	564.712425	18.910285	-0.042869	1.494414
223.505306	556.865180	18.915290	-0.042883	1.487007
223.180553	549.095722	18.920295	-0.042818	1.479570
223.222932	541.247253	18.925299	-0.042821	1.472077
223.303384	533.381919	18.930304	-0.042831	1.464536
223.017208	525.623750	18.935309	-0.042773	1.457001
223.006702	517.809907	18.940314	-0.042766	1.449417
222.985702	510.000289	18.945319	-0.042757	1.441796
222.837927	502.235957	18.950323	-0.042725	1.434157
222.687941	494.444739	18.955328	-0.042692	1.426451
222.679754	486.649490	18.960333	-0.042686	1.418723
222.764936	478.847426	18.965338	-0.042697	1.410960
222.526061	471.085675	18.970343	-0.042647	1.403142
222.453176	463.324556	18.975347	-0.042629	1.395307
222.535087	455.498826	18.980352	-0.042640	1.387389
222.124007	447.782674	18.985357	-0.042558	1.379454
221.939204	440.036339	18.990362	-0.042519	1.371481
221.960990	432.240534	18.995367	-0.042518	1.363445
221.927900	424.486919	19.000371	-0.042507	1.355395
221.877451	416.707749	19.005376	-0.042493	1.347268
221.617208	408.988052	19.010381	-0.042440	1.339118
221.685768	401.219300	19.015386	-0.042448	1.330923
221.491504	393.496274	19.020391	-0.042407	1.322680
221.355901	385.749773	19.025395	-0.042377	1.314370
221.419755	377.873530	19.030400	-0.042384	1.305904
221.363039	370.156115	19.035405	-0.042369	1.297532
221.161053	362.461141	19.040410	-0.042326	1.289105
220.857195	354.777077	19.045415	-0.042265	1.280614
221.056695	347.030849	19.050419	-0.042297	1.272092
220.805673	339.348687	19.055424	-0.042246	1.263500
220.597821	331.667863	19.060429	-0.042202	1.254858
220.891699	323.910497	19.065434	-0.042252	1.246165
220.418247	316.297753	19.070439	-0.042159	1.237428
220.302101	308.598630	19.075443	-0.042133	1.228600
220.327220	300.890817	19.080448	-0.042133	1.219725
219.897155	293.269773	19.085453	-0.042048	1.210796
219.806800	285.604600	19.090458	-0.042026	1.201816
219.744746	277.930036	19.095463	-0.042010	1.192763
219.916320	270.220849	19.100467	-0.042037	1.183648
219.625382	262.618140	19.105472	-0.041979	1.174494
219.430691	254.979641	19.110477	-0.041938	1.165246
219.468610	247.342315	19.115482	-0.041940	1.155973
219.375286	239.664755	19.120487	-0.041918	1.146548
219.163232	232.069380	19.125491	-0.041874	1.137121
219.108204	224.445872	19.130496	-0.041859	1.127614
219.055535	216.836942	19.135501	-0.041844	1.118045
218.879567	209.260984	19.140506	-0.041807	1.108409
218.550217	201.704628	19.145511	-0.041741	1.098679
218.658602	194.092057	19.150515	-0.041756	1.088887
218.543671	186.539986	19.155520	-0.041730	1.079035
217.940323	179.048079	19.160525	-0.041613	1.069060
218.045575	171.462356	19.165530	-0.041628	1.059029
217.824004	163.928642	19.170535	-0.041582	1.048896
217.684524	156.414219	19.175539	-0.041552	1.038709
217.445699	148.907676	19.180544	-0.041502	1.028409
217.357921	141.396986	19.185549	-0.041481	1.018035
217.216048	133.907584	19.190554	-0.041450	1.007571
217.211004	126.412041	19.195559	-0.041445	0.997022
217.152627	118.899570	19.200563	-0.041429	0.986322
216.884390	111.472703	19.205568	-0.041375	0.975576
216.600013	104.046280	19.210573	-0.041317	0.964707
216.465041	96.636140	19.215578	-0.041288	0.953776
216.227715	89.232570	19.220583	-0.041239	0.942702
215.902466	81.866794	19.225587	-0.041174	0.931529
216.002193	74.452474	19.230592	-0.041188	0.920261
215.828450	67.094139	19.235597	-0.041151	0.908865
215.611347	59.998107	19.240602	-0.041106	0.897725