Thu Mar 11 18:07:45 2021

Number of Points = 3620
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.598788	0.064133	0.000000	0.000073	0.723626

0.911115	0.008056	0.005005	0.000015	0.723626
0.695000	0.045268	0.010010	0.000055	0.723624
0.812021	0.028066	0.015014	0.000033	0.723631
0.689131	-0.067265	0.020019	0.000056	0.723401
0.704530	-0.105667	0.025024	0.000053	0.723332
0.712628	-0.106981	0.030029	0.000051	0.723332
0.711766	-0.108411	0.035034	0.000051	0.723330
0.855408	-0.131550	0.040038	0.000024	0.723335
0.727808	-0.114117	0.045043	0.000048	0.723325
0.689673	-0.102542	0.050048	0.000055	0.723334
0.786595	-0.122417	0.055053	0.000037	0.723329
0.730543	-0.111513	0.060058	0.000047	0.723332
0.887349	-0.137274	0.065062	0.000018	0.723336
0.769403	-0.122516	0.070067	0.000040	0.723324
0.791538	-0.119841	0.075072	0.000035	0.723337
0.810015	-0.125232	0.080077	0.000032	0.723334
0.952089	-0.191717	0.085082	0.000005	0.723253
0.997241	-0.326893	0.090086	-0.000003	0.723004
0.800224	-0.296064	0.095091	0.000033	0.722996
0.872013	-0.308479	0.100096	0.000020	0.722997
0.860206	-0.307005	0.105101	0.000022	0.722996
0.998072	-0.332181	0.110106	-0.000004	0.722995
0.941709	-0.336420	0.115110	0.000006	0.722967
0.892730	-0.473281	0.120115	0.000015	0.722682
0.897773	-0.470949	0.125120	0.000014	0.722689
0.868399	-0.466387	0.130125	0.000019	0.722688
0.763541	-0.450333	0.135130	0.000039	0.722683
1.048262	-0.544090	0.140134	-0.000014	0.722599
1.003087	-0.658935	0.145139	-0.000006	0.722358
0.943912	-0.644772	0.150144	0.000005	0.722365
0.799994	-0.618224	0.155149	0.000032	0.722367
0.756411	-0.644562	0.160154	0.000039	0.722301
0.891427	-0.785242	0.165158	0.000014	0.722072
0.707266	-0.756177	0.170163	0.000048	0.722065
0.908185	-0.787892	0.175168	0.000011	0.722073
0.896382	-0.871644	0.180173	0.000013	0.721905
0.762179	-0.933621	0.185178	0.000038	0.721736
0.931334	-0.960079	0.190182	0.000006	0.721744
0.698073	-0.950230	0.195187	0.000049	0.721682
0.814584	-1.095177	0.200192	0.000028	0.721438
0.688634	-1.073933	0.205197	0.000051	0.721436
0.691196	-1.083354	0.210202	0.000050	0.721419
0.893497	-1.269449	0.215206	0.000013	0.721124
0.603851	-1.224133	0.220211	0.000066	0.721112
0.766402	-1.269579	0.225216	0.000036	0.721080
0.753454	-1.372528	0.230221	0.000038	0.720873
0.557025	-1.340317	0.235226	0.000075	0.720868
0.717712	-1.433463	0.240230	0.000045	0.720741
0.779371	-1.551353	0.245235	0.000033	0.720531
0.595662	-1.516727	0.250240	0.000067	0.720535
0.501837	-1.631830	0.255245	0.000085	0.720276
0.583175	-1.677977	0.260250	0.000069	0.720214
0.839273	-1.776762	0.265254	0.000021	0.720109
0.573401	-1.843203	0.270259	0.000071	0.719885
0.611608	-1.845008	0.275264	0.000064	0.719896
0.434295	-1.962748	0.280269	0.000097	0.719602
0.067051	-1.902881	0.285274	0.000165	0.719591
-0.023675	-1.979882	0.290278	0.000182	0.719408
-2.010114	-1.702933	0.295283	0.000551	0.719257
-2.392141	-1.630653	0.300288	0.000622	0.719265
-2.651704	-1.626568	0.305293	0.000670	0.719182
-3.494662	-1.593631	0.310298	0.000827	0.718952
-2.993594	-1.678947	0.315302	0.000734	0.718960
-3.623335	-1.572361	0.320307	0.000851	0.718949
-3.832509	-1.535851	0.325312	0.000889	0.718948
-4.285077	-1.613646	0.330317	0.000973	0.718635
-4.592219	-1.560082	0.335322	0.001030	0.718633
-4.245921	-1.617639	0.340326	0.000966	0.718642
-4.602279	-1.558869	0.345331	0.001032	0.718633
-4.742207	-1.540108	0.350336	0.001058	0.718621
-5.073415	-1.620429	0.355341	0.001119	0.718346
-5.540021	-1.538620	0.360346	0.001206	0.718344
-5.491783	-1.542382	0.365350	0.001197	0.718354
-5.583479	-1.530351	0.370355	0.001214	0.718346
-5.486957	-1.546152	0.375360	0.001196	0.718349
-5.702299	-1.597820	0.380365	0.001236	0.718171
-6.564251	-1.528211	0.385370	0.001396	0.718006
-6.228915	-1.582400	0.390374	0.001334	0.718017
-6.832803	-1.479890	0.395379	0.001446	0.718007
-6.569168	-1.523956	0.400384	0.001397	0.718013
-6.232634	-1.584522	0.405389	0.001334	0.718012
-6.705820	-1.584926	0.410394	0.001422	0.717845
-7.577220	-1.502021	0.415398	0.001584	0.717703
-7.175946	-1.577673	0.420403	0.001509	0.717695
-7.455750	-1.524354	0.425408	0.001561	0.717702
-7.650186	-1.490978	0.430413	0.001597	0.717700
-7.533686	-1.513814	0.435418	0.001575	0.717696
-7.056418	-1.605135	0.440422	0.001486	0.717684
-8.116893	-1.574233	0.445427	0.001683	0.717372
-8.451159	-1.510936	0.450432	0.001745	0.717380
-8.523250	-1.499549	0.455437	0.001759	0.717377
-8.567225	-1.495025	0.460442	0.001767	0.717371
-8.628365	-1.481009	0.465446	0.001778	0.717377
-8.543198	-1.499251	0.470451	0.001762	0.717371
-8.428604	-1.517485	0.475456	0.001740	0.717376
-8.877719	-1.567549	0.480461	0.001824	0.717119
-9.337578	-1.506778	0.485466	0.001909	0.717078
-9.206498	-1.526884	0.490470	0.001885	0.717084
-9.247120	-1.522443	0.495475	0.001892	0.717079
-9.453354	-1.485503	0.500480	0.001930	0.717080
-8.992446	-1.566964	0.505485	0.001844	0.717081
-9.210396	-1.554765	0.510490	0.001885	0.717029
-9.975082	-1.556594	0.515494	0.002027	0.716756
-9.974920	-1.562177	0.520499	0.002027	0.716745
-10.207023	-1.518420	0.525504	0.002070	0.716750
-10.125795	-1.533198	0.530509	0.002055	0.716750
-10.437666	-1.480635	0.535514	0.002113	0.716745
-9.840500	-1.581637	0.540518	0.002001	0.716755
-10.239865	-1.552132	0.545523	0.002075	0.716673
-11.168673	-1.503643	0.550528	0.002248	0.716442
-10.985865	-1.535964	0.555533	0.002214	0.716443
-11.478004	-1.452509	0.560538	0.002305	0.716435
-11.196571	-1.497314	0.565542	0.002253	0.716446
-11.097613	-1.520413	0.570547	0.002234	0.716435
-11.215494	-1.495466	0.575552	0.002256	0.716443
-11.463810	-1.451739	0.580557	0.002302	0.716443
-11.423990	-1.568936	0.585562	0.002295	0.716225
-11.946152	-1.525756	0.590566	0.002392	0.716126
-12.243708	-1.475186	0.595571	0.002447	0.716122
-12.215759	-1.476534	0.600576	0.002442	0.716129
-12.075794	-1.501618	0.605581	0.002415	0.716129
-12.179126	-1.485725	0.610586	0.002434	0.716125
-12.097182	-1.497203	0.615590	0.002419	0.716131
-12.314907	-1.493907	0.620595	0.002459	0.716061
-12.961761	-1.470092	0.625600	0.002580	0.715880
-12.852153	-1.491699	0.630605	0.002559	0.715876
-13.079992	-1.453389	0.635610	0.002601	0.715872
-12.615778	-1.532296	0.640614	0.002515	0.715880
-12.852137	-1.495226	0.645619	0.002559	0.715870
-13.164475	-1.437689	0.650624	0.002617	0.715874
-12.654870	-1.575287	0.655629	0.002522	0.715782
-13.588800	-1.534147	0.660634	0.002695	0.715534
-13.624060	-1.524435	0.665638	0.002702	0.715541
-14.130828	-1.437103	0.670643	0.002796	0.715536
-13.411835	-1.562976	0.675648	0.002662	0.715540
-13.670714	-1.517836	0.680653	0.002710	0.715539
-13.959881	-1.468048	0.685658	0.002764	0.715535
-13.680081	-1.595661	0.690662	0.002711	0.715382
-14.746306	-1.486260	0.695667	0.002910	0.715222
-14.779397	-1.478706	0.700672	0.002916	0.715226
-14.555417	-1.516791	0.705677	0.002874	0.715230
-14.874161	-1.463621	0.710682	0.002933	0.715223
-14.929435	-1.448692	0.715686	0.002943	0.715233
-15.080325	-1.426802	0.720691	0.002971	0.715223
-14.723219	-1.507764	0.725696	0.002905	0.715189
-15.436165	-1.524085	0.730701	0.003037	0.714905
-16.149263	-1.399910	0.735706	0.003170	0.714900
-15.920791	-1.437656	0.740710	0.003127	0.714906
-15.437239	-1.528947	0.745715	0.003037	0.714896
-15.922470	-1.439390	0.750720	0.003127	0.714903
-15.790786	-1.462017	0.755725	0.003102	0.714905
-15.604651	-1.498789	0.760730	0.003068	0.714898
-15.577276	-1.586787	0.765734	0.003062	0.714733
-16.724835	-1.448188	0.770739	0.003276	0.714603
-16.201288	-1.541258	0.775744	0.003178	0.714603
-16.160592	-1.547558	0.780749	0.003170	0.714605
-16.803549	-1.437723	0.785754	0.003290	0.714596
-16.237652	-1.531812	0.790758	0.003184	0.714610
-16.218328	-1.540870	0.795763	0.003181	0.714599
-17.468156	-1.472099	0.800768	0.003413	0.714294
-17.536457	-1.471201	0.805773	0.003426	0.714272
-17.398196	-1.498971	0.810778	0.003400	0.714266
-17.306545	-1.509753	0.815782	0.003383	0.714277
-17.697282	-1.445359	0.820787	0.003455	0.714267
-17.422738	-1.492144	0.825792	0.003404	0.714272
-17.381660	-1.498356	0.830797	0.003396	0.714274
-17.777897	-1.493365	0.835802	0.003470	0.714144
-18.757403	-1.407145	0.840806	0.003652	0.713969
-18.393189	-1.478351	0.845811	0.003584	0.713957
-18.809323	-1.403263	0.850816	0.003661	0.713959
-18.681285	-1.424694	0.855821	0.003637	0.713962
-17.990164	-1.551355	0.860826	0.003509	0.713955
-18.140879	-1.519627	0.865830	0.003536	0.713965
-18.699592	-1.424516	0.870835	0.003640	0.713957
-18.584559	-1.575797	0.875840	0.003619	0.713697
-19.054048	-1.518720	0.880845	0.003706	0.713645
-19.565869	-1.430311	0.885850	0.003801	0.713639
-19.253608	-1.480522	0.890854	0.003743	0.713650
-19.369656	-1.464590	0.895859	0.003764	0.713641
-19.312378	-1.470628	0.900864	0.003753	0.713650
-19.314760	-1.469884	0.905869	0.003754	0.713651
-19.719446	-1.507867	0.910874	0.003829	0.713432
-20.473032	-1.410205	0.915878	0.003969	0.713360
-20.699408	-1.373397	0.920883	0.004011	0.713353
-20.335515	-1.437363	0.925888	0.003943	0.713355
-20.083671	-1.482738	0.930893	0.003896	0.713354
-20.700580	-1.375642	0.935898	0.004011	0.713349
-20.574047	-1.395356	0.940902	0.003987	0.713355
-20.359344	-1.437723	0.945907	0.003947	0.713347
-20.853378	-1.484329	0.950912	0.004039	0.713079
-21.668792	-1.369746	0.955917	0.004190	0.713019
-21.582640	-1.388895	0.960922	0.004174	0.713011
-20.828976	-1.518859	0.965926	0.004034	0.713020
-21.638364	-1.379817	0.970931	0.004184	0.713010
-21.749303	-1.358515	0.975936	0.004205	0.713014
-21.055759	-1.480316	0.980941	0.004076	0.713017
-21.573229	-1.391993	0.985946	0.004172	0.713010
-21.865656	-1.473824	0.990950	0.004226	0.712744
-22.336406	-1.412167	0.995955	0.004314	0.712700
-22.514799	-1.379592	1.000960	0.004347	0.712702
-22.349904	-1.406967	1.005965	0.004316	0.712706
-22.570821	-1.372224	1.010970	0.004357	0.712697
-22.221289	-1.430186	1.015974	0.004291	0.712706
-22.372003	-1.407089	1.020979	0.004319	0.712699
-22.505496	-1.392862	1.025984	0.004344	0.712680
-22.655868	-1.515102	1.030989	0.004372	0.712384
-22.940507	-1.467827	1.035994	0.004425	0.712377
-23.341393	-1.392276	1.040998	0.004499	0.712386
-22.911378	-1.474024	1.046003	0.004419	0.712376
-22.959624	-1.462875	1.051008	0.004428	0.712381
-23.195844	-1.419721	1.056013	0.004472	0.712383
-23.384442	-1.400020	1.061018	0.004507	0.712356
-23.531797	-1.508431	1.066022	0.004534	0.712088
-24.152166	-1.400900	1.071027	0.004649	0.712082
-24.552385	-1.329423	1.076032	0.004724	0.712083
-23.812359	-1.458892	1.081037	0.004586	0.712088
-24.070100	-1.416720	1.086042	0.004633	0.712081
-24.214485	-1.385974	1.091046	0.004660	0.712091
-24.135623	-1.403858	1.096051	0.004645	0.712084
-24.476557	-1.462884	1.101056	0.004709	0.711845
-25.316395	-1.358364	1.106061	0.004865	0.711756
-25.421947	-1.342643	1.111066	0.004884	0.711750
-24.771949	-1.453059	1.116070	0.004763	0.711761
-25.104772	-1.397701	1.121075	0.004825	0.711753
-25.139241	-1.390222	1.126080	0.004831	0.711756
-24.634765	-1.478427	1.131085	0.004737	0.711760
-24.989163	-1.458367	1.136090	0.004803	0.711674
-26.120332	-1.368052	1.141094	0.005013	0.711453
-25.773695	-1.432672	1.146099	0.004949	0.711447
-25.840857	-1.419447	1.151104	0.004961	0.711450
-25.802486	-1.423970	1.156109	0.004954	0.711455
-26.078750	-1.379979	1.161114	0.005005	0.711445
-25.847356	-1.417294	1.166118	0.004962	0.711453
-25.996099	-1.394813	1.171123	0.004989	0.711445
-26.813943	-1.401006	1.176128	0.005142	0.711142
-26.758168	-1.416063	1.181133	0.005131	0.711133
-27.038672	-1.368575	1.186138	0.005183	0.711128
-26.780675	-1.411181	1.191142	0.005135	0.711135
-26.996016	-1.376087	1.196147	0.005175	0.711129
-26.875404	-1.397731	1.201152	0.005152	0.711129
-26.581983	-1.447041	1.206157	0.005097	0.711135
-26.989204	-1.457801	1.211162	0.005173	0.710969
-27.456717	-1.427499	1.216166	0.005260	0.710863
-27.243875	-1.468472	1.221171	0.005220	0.710858
-27.566732	-1.408587	1.226176	0.005280	0.710863
-27.523269	-1.413903	1.231181	0.005272	0.710868
-27.450060	-1.431009	1.236186	0.005258	0.710860
-27.363825	-1.464354	1.241190	0.005242	0.710824
-28.343797	-1.442253	1.246195	0.005424	0.710520
-28.444203	-1.422323	1.251200	0.005443	0.710524
-28.373093	-1.432685	1.256205	0.005429	0.710529
-28.762950	-1.366878	1.261210	0.005502	0.710522
-28.337292	-1.437960	1.266214	0.005422	0.710532
-28.559398	-1.402164	1.271219	0.005464	0.710525
-28.724687	-1.373719	1.276224	0.005494	0.710523
-28.867850	-1.500009	1.281229	0.005521	0.710220
-29.162535	-1.454870	1.286234	0.005575	0.710206
-29.399965	-1.408530	1.291238	0.005619	0.710214
-29.584231	-1.378420	1.296243	0.005654	0.710209
-29.560853	-1.383479	1.301248	0.005649	0.710207
-29.279932	-1.430881	1.306253	0.005597	0.710213
-29.664390	-1.365916	1.311258	0.005668	0.710206
-29.750733	-1.491876	1.316262	0.005684	0.709924
-30.200945	-1.431781	1.321267	0.005768	0.709884
-30.469863	-1.383265	1.326272	0.005818	0.709886
-30.287350	-1.414537	1.331277	0.005783	0.709888
-30.382498	-1.403118	1.336282	0.005801	0.709878
-30.388427	-1.396904	1.341286	0.005802	0.709888
-30.367431	-1.402748	1.346291	0.005798	0.709884
-30.714625	-1.447930	1.351296	0.005862	0.709671
-31.212397	-1.399953	1.356301	0.005955	0.709589
-31.467419	-1.360078	1.361306	0.006002	0.709579
-31.101557	-1.418526	1.366310	0.005934	0.709592
-31.213203	-1.400028	1.371315	0.005955	0.709590
-31.387062	-1.369702	1.376320	0.005987	0.709589
-31.232636	-1.395540	1.381325	0.005958	0.709592
-31.347318	-1.440567	1.386330	0.005979	0.709462
-32.200408	-1.388927	1.391334	0.006138	0.709261
-32.321441	-1.370745	1.396339	0.006160	0.709255
-32.589989	-1.321397	1.401344	0.006210	0.709258
-32.082829	-1.409907	1.406349	0.006115	0.709262
-32.169264	-1.399099	1.411354	0.006131	0.709253
-32.421413	-1.350216	1.416358	0.006178	0.709261
-32.282689	-1.376495	1.421363	0.006152	0.709259
-32.768472	-1.414420	1.426368	0.006242	0.709010
-33.302831	-1.347403	1.431373	0.006342	0.708953
-33.043091	-1.397394	1.436378	0.006293	0.708946
-32.632710	-1.467528	1.441382	0.006217	0.708953
-33.179085	-1.373926	1.446387	0.006318	0.708945
-33.141265	-1.380116	1.451392	0.006311	0.708947
-32.613634	-1.470757	1.456397	0.006213	0.708954
-33.502272	-1.445126	1.461402	0.006378	0.708688
-34.271217	-1.336011	1.466406	0.006521	0.708633
-33.840206	-1.415786	1.471411	0.006441	0.708627
-33.888519	-1.404521	1.476416	0.006449	0.708633
-34.032568	-1.377634	1.481421	0.006476	0.708636
-34.127800	-1.364124	1.486426	0.006494	0.708629
-33.920160	-1.397153	1.491430	0.006455	0.708637
-34.181037	-1.420042	1.496435	0.006503	0.708498
-35.015996	-1.349009	1.501440	0.006658	0.708343
-34.313394	-1.473880	1.506445	0.006528	0.708344
-34.876341	-1.378058	1.511450	0.006632	0.708335
-34.708780	-1.402855	1.516454	0.006601	0.708346
-34.524228	-1.438625	1.521459	0.006566	0.708340
-34.826939	-1.385174	1.526464	0.006623	0.708339
-35.025721	-1.473143	1.531469	0.006659	0.708092
-35.792493	-1.382488	1.536474	0.006802	0.708000
-35.524094	-1.427247	1.541478	0.006752	0.708007
-35.648744	-1.407867	1.546483	0.006775	0.708002
-35.985937	-1.350058	1.551488	0.006838	0.707997
-35.372572	-1.457354	1.556493	0.006723	0.708002
-35.776266	-1.387888	1.561498	0.006798	0.707997
-36.075404	-1.450396	1.566502	0.006854	0.707765
-36.835279	-1.352268	1.571507	0.006995	0.707690
-36.586524	-1.397614	1.576512	0.006949	0.707689
-36.391488	-1.430777	1.581517	0.006912	0.707692
-36.872656	-1.350144	1.586522	0.007002	0.707682
-36.625563	-1.389240	1.591526	0.006955	0.707693
-36.746283	-1.368808	1.596531	0.006978	0.707691
-37.016896	-1.377762	1.601536	0.007028	0.707576
-37.521711	-1.388835	1.606541	0.007122	0.707374
-37.505504	-1.397125	1.611546	0.007119	0.707363
-37.901415	-1.322429	1.616550	0.007192	0.707372
-37.504005	-1.397267	1.621555	0.007118	0.707364
-37.570172	-1.384924	1.626560	0.007130	0.707365
-37.777400	-1.345493	1.631565	0.007169	0.707371
-37.747814	-1.357101	1.636570	0.007163	0.707358
-37.628315	-1.491864	1.641574	0.007141	0.707131
-38.554720	-1.356314	1.646579	0.007313	0.707072
-38.598401	-1.350739	1.651584	0.007321	0.707068
-38.122126	-1.431821	1.656589	0.007232	0.707076
-38.668323	-1.339394	1.661594	0.007333	0.707066
-38.557460	-1.354525	1.666598	0.007313	0.707076
-38.224555	-1.415999	1.671603	0.007251	0.707072
-38.686432	-1.474558	1.676608	0.007336	0.706789
-39.610312	-1.332173	1.681613	0.007508	0.706745
-39.440736	-1.365932	1.686618	0.007477	0.706738
-38.998712	-1.439358	1.691622	0.007394	0.706749
-39.412518	-1.369826	1.696627	0.007471	0.706741
-39.383450	-1.374576	1.701632	0.007465	0.706742
-39.145394	-1.413936	1.706637	0.007421	0.706748
-39.757398	-1.431138	1.711642	0.007535	0.706495
-40.562294	-1.314533	1.716646	0.007684	0.706441
-40.356160	-1.355196	1.721651	0.007646	0.706434
-40.307914	-1.364647	1.726656	0.007637	0.706432
-40.456386	-1.333671	1.731661	0.007664	0.706442
-40.324836	-1.362088	1.736666	0.007640	0.706432
-39.859391	-1.441052	1.741670	0.007553	0.706440
-40.280119	-1.434515	1.746675	0.007631	0.706303
-41.466616	-1.313081	1.751680	0.007852	0.706122
-40.603544	-1.463746	1.756685	0.007691	0.706129
-41.019448	-1.394494	1.761690	0.007768	0.706119
-41.255259	-1.350279	1.766694	0.007812	0.706124
-40.982735	-1.401457	1.771699	0.007761	0.706119
-41.098953	-1.380852	1.776704	0.007782	0.706119
-41.091281	-1.454180	1.781709	0.007781	0.705975
-41.922215	-1.367368	1.786714	0.007935	0.705852
-41.777532	-1.390439	1.791718	0.007908	0.705858
-41.917015	-1.365764	1.796723	0.007934	0.705858
-42.203010	-1.314816	1.801728	0.007987	0.705858
-41.593517	-1.422687	1.806733	0.007874	0.705860
-41.679687	-1.411008	1.811738	0.007890	0.705853
-42.381454	-1.424408	1.816742	0.008020	0.705574
-42.754434	-1.384366	1.821747	0.008089	0.705521
-42.678834	-1.397723	1.826752	0.008075	0.705522
-42.630954	-1.402763	1.831757	0.008066	0.705529
-42.694224	-1.396717	1.836762	0.008078	0.705519
-42.857162	-1.364524	1.841766	0.008108	0.705526
-42.798069	-1.375287	1.846771	0.008097	0.705525
-43.721967	-1.370921	1.851776	0.008269	0.705203
-43.458617	-1.413057	1.856781	0.008219	0.705213
-43.711596	-1.373304	1.861786	0.008266	0.705203
-43.919630	-1.332841	1.866790	0.008305	0.705210
-43.883500	-1.340712	1.871795	0.008298	0.705207
-43.755406	-1.365094	1.876800	0.008274	0.705204
-43.667967	-1.378469	1.881805	0.008258	0.705209
-44.085037	-1.407529	1.886810	0.008335	0.705001
-44.544478	-1.384482	1.891814	0.008420	0.704883
-44.358636	-1.418113	1.896819	0.008386	0.704882
-44.805167	-1.340286	1.901824	0.008469	0.704879
-44.552380	-1.380814	1.906829	0.008421	0.704888
-44.504405	-1.394323	1.911834	0.008412	0.704879
-44.750926	-1.346147	1.916838	0.008458	0.704887
-44.770716	-1.425334	1.921843	0.008462	0.704721
-45.402501	-1.383079	1.926848	0.008579	0.704580
-45.042150	-1.443522	1.931853	0.008512	0.704588
-45.603833	-1.347565	1.936858	0.008616	0.704579
-45.240494	-1.409510	1.941862	0.008548	0.704585
-45.107040	-1.433375	1.946867	0.008523	0.704586
-45.616287	-1.344907	1.951872	0.008618	0.704581
-45.849508	-1.446716	1.956877	0.008661	0.704293
-46.188086	-1.407991	1.961882	0.008724	0.704249
-46.518275	-1.347261	1.966886	0.008786	0.704253
-46.234724	-1.398468	1.971891	0.008733	0.704252
-46.358486	-1.379109	1.976896	0.008755	0.704247
-46.355161	-1.376447	1.981901	0.008755	0.704254
-46.492628	-1.355303	1.986906	0.008780	0.704248
-46.656341	-1.442035	1.991910	0.008811	0.704014
-47.244175	-1.372906	1.996915	0.008920	0.703942
-47.397338	-1.344158	2.001920	0.008948	0.703946

-47.459465	-1.334894	2.011917	0.008959	0.703943
-47.401324	-1.343934	2.021914	0.008948	0.703946
-47.363297	-1.352410	2.031910	0.008941	0.703943
-47.303352	-1.362392	2.041907	0.008929	0.703945
-47.349732	-1.353611	2.051904	0.008938	0.703947
-47.430655	-1.341306	2.061901	0.008952	0.703943
-47.418717	-1.343853	2.071898	0.008950	0.703943
-47.243165	-1.374640	2.081894	0.008917	0.703944
-47.299292	-1.364082	2.091891	0.008927	0.703946
-47.167029	-1.389244	2.101888	0.008902	0.703944
-47.303769	-1.367917	2.111885	0.008927	0.703938
-47.436840	-1.343486	2.121882	0.008952	0.703940
-47.169761	-1.390281	2.131878	0.008902	0.703942
-46.791267	-1.347508	2.141875	0.008831	0.704165
-46.519357	-1.354233	2.151872	0.008780	0.704250
-46.274100	-1.398027	2.161869	0.008734	0.704251
-46.743136	-1.314785	2.171866	0.008821	0.704250
-46.439845	-1.357375	2.181862	0.008764	0.704274
-45.844430	-1.309786	2.191859	0.008653	0.704585
-45.729427	-1.331211	2.201856	0.008631	0.704583
-45.568972	-1.361593	2.211853	0.008601	0.704580
-45.742081	-1.307996	2.221850	0.008633	0.704627
-44.692140	-1.368943	2.231846	0.008437	0.704882
-44.810760	-1.346934	2.241843	0.008459	0.704884
-44.563790	-1.390876	2.251840	0.008413	0.704885
-44.706449	-1.327216	2.261837	0.008439	0.704963
-43.970376	-1.337692	2.271834	0.008301	0.705206
-43.602674	-1.404321	2.281830	0.008233	0.705205
-43.795232	-1.368937	2.291827	0.008268	0.705207
-43.526423	-1.346932	2.301824	0.008218	0.705349
-42.886351	-1.375563	2.311821	0.008098	0.705521
-42.905145	-1.373019	2.321818	0.008102	0.705520
-42.670211	-1.413882	2.331814	0.008058	0.705523
-42.349398	-1.369221	2.341811	0.007997	0.705729
-41.697489	-1.421087	2.351808	0.007876	0.705859
-41.975669	-1.371294	2.361805	0.007927	0.705860
-41.894034	-1.386770	2.371802	0.007912	0.705858
-41.349951	-1.383295	2.381798	0.007810	0.706061
-41.364783	-1.348420	2.391795	0.007813	0.706127
-41.080816	-1.398332	2.401792	0.007759	0.706129
-41.127102	-1.336815	2.411789	0.007768	0.706236
-40.255197	-1.391214	2.421786	0.007605	0.706440
-40.510215	-1.344890	2.431782	0.007652	0.706442
-40.485469	-1.347658	2.441779	0.007647	0.706446
-39.785161	-1.324168	2.451776	0.007517	0.706745
-39.638870	-1.351091	2.461773	0.007489	0.706744
-39.557100	-1.364762	2.471770	0.007473	0.706746
-39.194878	-1.305576	2.481766	0.007406	0.706995
-38.987591	-1.301919	2.491763	0.007367	0.707077
-38.592483	-1.372259	2.501760	0.007293	0.707078
-38.641641	-1.289288	2.511757	0.007302	0.707228
-37.725807	-1.383097	2.521754	0.007131	0.707368
-37.781401	-1.374229	2.531750	0.007141	0.707366
-37.577615	-1.410076	2.541747	0.007103	0.707368
-37.001602	-1.366244	2.551744	0.006995	0.707662
-36.985925	-1.356016	2.561741	0.006992	0.707689
-36.661123	-1.414873	2.571738	0.006931	0.707688
-36.846181	-1.331109	2.581734	0.006965	0.707790
-35.982322	-1.377275	2.591731	0.006804	0.708007
-35.799532	-1.410897	2.601728	0.006770	0.708005
-36.086107	-1.361836	2.611725	0.006823	0.708002
-35.332406	-1.359320	2.621722	0.006682	0.708277
-35.298576	-1.332427	2.631718	0.006675	0.708344
-34.867988	-1.409786	2.641715	0.006595	0.708343
-35.004342	-1.357198	2.651712	0.006620	0.708400
-34.484883	-1.334542	2.661709	0.006523	0.708632
-34.254881	-1.376149	2.671706	0.006480	0.708631
-34.502328	-1.331880	2.681702	0.006526	0.708632
-33.682782	-1.333824	2.691699	0.006373	0.708921
-33.543589	-1.345077	2.701696	0.006346	0.708949
-33.510917	-1.349953	2.711693	0.006340	0.708951
-33.023836	-1.353250	2.721690	0.006249	0.709119
-32.574279	-1.364014	2.731686	0.006165	0.709259
-32.399548	-1.395066	2.741683	0.006132	0.709259
-32.424789	-1.389893	2.751680	0.006137	0.709261
-32.081153	-1.302464	2.761677	0.006072	0.709559
-31.606235	-1.373575	2.771674	0.005984	0.709587
-31.519552	-1.388700	2.781670	0.005967	0.709588
-31.396043	-1.342594	2.791667	0.005944	0.709725
-30.573286	-1.406590	2.801664	0.005790	0.709891
-30.646333	-1.394382	2.811661	0.005804	0.709890
-30.703211	-1.384938	2.821658	0.005814	0.709889
-30.209027	-1.350827	2.831654	0.005721	0.710134
-29.848866	-1.374372	2.841651	0.005654	0.710216
-29.935537	-1.358485	2.851648	0.005670	0.710217
-29.735397	-1.352998	2.861645	0.005632	0.710300
-28.754043	-1.415800	2.871642	0.005449	0.710525
-28.925078	-1.385114	2.881638	0.005481	0.710526
-28.892104	-1.390900	2.891635	0.005474	0.710527
-28.671242	-1.313207	2.901632	0.005433	0.710761
-28.061221	-1.372939	2.911629	0.005319	0.710859
-28.243881	-1.340847	2.921626	0.005353	0.710859
-27.987126	-1.349597	2.931622	0.005305	0.710934
-27.309435	-1.371253	2.941619	0.005178	0.711132
-27.431038	-1.350277	2.951616	0.005200	0.711131
-27.446811	-1.349256	2.961613	0.005203	0.711128
-26.590717	-1.346655	2.971610	0.005043	0.711438
-26.471218	-1.363588	2.981606	0.005021	0.711448
-26.201160	-1.411503	2.991603	0.004970	0.711449
-26.273834	-1.323195	3.001600	0.004983	0.711600
-25.567245	-1.372240	3.011597	0.004852	0.711753
-25.614378	-1.364338	3.021594	0.004860	0.711753
-25.670595	-1.336005	3.031590	0.004870	0.711790
-24.622762	-1.373685	3.041587	0.004675	0.712088
-24.564961	-1.383776	3.051584	0.004664	0.712089
-24.401730	-1.413908	3.061581	0.004633	0.712087
-24.607254	-1.315467	3.071578	0.004671	0.712211
-23.672522	-1.397477	3.081574	0.004497	0.712380
-23.758373	-1.380716	3.091571	0.004512	0.712384
-23.736770	-1.384632	3.101568	0.004508	0.712384
-22.923161	-1.373923	3.111565	0.004356	0.712695
-22.969342	-1.362817	3.121562	0.004364	0.712701
-22.698560	-1.409051	3.131558	0.004314	0.712706
-22.741564	-1.341632	3.141555	0.004321	0.712825
-21.896140	-1.394098	3.151552	0.004164	0.713021
-21.873529	-1.400235	3.161549	0.004159	0.713018
-21.987628	-1.381895	3.171546	0.004180	0.713014
-21.191593	-1.387861	3.181542	0.004031	0.713285
-21.019669	-1.385323	3.191539	0.003999	0.713352
-20.961309	-1.395316	3.201536	0.003988	0.713353
-20.984755	-1.374585	3.211533	0.003992	0.713387
-20.507242	-1.332173	3.221530	0.003903	0.713641
-20.055271	-1.411350	3.231526	0.003818	0.713644
-20.136453	-1.396205	3.241523	0.003833	0.713646
-19.635030	-1.382339	3.251520	0.003739	0.713852
-19.217750	-1.400641	3.261517	0.003661	0.713964
-19.373659	-1.374030	3.271514	0.003690	0.713962
-19.173976	-1.393746	3.281510	0.003653	0.713994
-18.473338	-1.378575	3.291507	0.003522	0.714273
-18.401331	-1.391548	3.301504	0.003508	0.714273
-18.143788	-1.438953	3.311501	0.003460	0.714271
-18.216344	-1.342641	3.321498	0.003473	0.714437
-17.027068	-1.472253	3.331494	0.003251	0.714601
-17.368963	-1.410188	3.341491	0.003315	0.714604
-17.328323	-1.416785	3.351488	0.003307	0.714606
-16.675208	-1.425776	3.361485	0.003185	0.714820
-16.592511	-1.399585	3.371482	0.003169	0.714902
-16.324048	-1.446059	3.381478	0.003119	0.714905
-16.342799	-1.443217	3.391475	0.003122	0.714904
-15.941802	-1.355206	3.401472	0.003047	0.715221
-15.567174	-1.419213	3.411469	0.002977	0.715227
-15.684226	-1.399647	3.421466	0.002998	0.715226
-15.188210	-1.403522	3.431462	0.002906	0.715394
-14.600153	-1.433508	3.441459	0.002796	0.715543
-14.353198	-1.478039	3.451456	0.002750	0.715542
-14.695070	-1.418148	3.461453	0.002813	0.715541
-14.174977	-1.385465	3.471450	0.002716	0.715790
-13.700278	-1.428218	3.481446	0.002627	0.715873
-13.559205	-1.451678	3.491443	0.002601	0.715877
-13.533319	-1.454186	3.501440	0.002595	0.715882
-13.180958	-1.394793	3.511437	0.002529	0.716125
-12.605920	-1.499186	3.521434	0.002422	0.716121
-12.831305	-1.455946	3.531430	0.002464	0.716128
-12.836775	-1.375619	3.541427	0.002464	0.716286
-11.963015	-1.450591	3.551424	0.002301	0.716446
-12.288287	-1.394056	3.561421	0.002362	0.716444
-11.819298	-1.466099	3.571418	0.002274	0.716467
-11.208851	-1.433185	3.581414	0.002160	0.716748
-10.996724	-1.471114	3.591411	0.002120	0.716749
-11.051297	-1.461221	3.601408	0.002130	0.716750
-10.842608	-1.410675	3.611405	0.002091	0.716924
-10.128787	-1.459169	3.621402	0.001958	0.717080
-10.219496	-1.441931	3.631398	0.001974	0.717083
-10.276555	-1.431199	3.641395	0.001985	0.717084
-9.461826	-1.428573	3.651392	0.001833	0.717377
-9.508703	-1.422619	3.661389	0.001841	0.717373
-9.513462	-1.422586	3.671386	0.001842	0.717372
-8.983023	-1.422035	3.681382	0.001742	0.717561
-8.720890	-1.400948	3.691379	0.001693	0.717695
-8.196931	-1.492282	3.701376	0.001596	0.717700
-8.385029	-1.459950	3.711373	0.001630	0.717698
-7.505824	-1.460321	3.721370	0.001466	0.718007
-7.645113	-1.434785	3.731366	0.001492	0.718009
-7.124627	-1.525813	3.741363	0.001395	0.718013
-7.449009	-1.430243	3.751360	0.001455	0.718089
-6.479193	-1.471317	3.761357	0.001274	0.718349
-6.307593	-1.502023	3.771354	0.001242	0.718349
-6.475417	-1.472988	3.781350	0.001272	0.718348
-6.148916	-1.484144	3.791347	0.001211	0.718442
-5.450601	-1.506921	3.801344	0.001081	0.718643
-5.406585	-1.514824	3.811341	0.001073	0.718643
-5.494236	-1.499831	3.821338	0.001089	0.718643
-5.245687	-1.464452	3.831334	0.001042	0.718801
-4.341868	-1.546312	3.841331	0.000873	0.718957
-4.474217	-1.522844	3.851328	0.000898	0.718958
-4.482098	-1.521584	3.861325	0.000899	0.718958
-4.109118	-1.480908	3.871322	0.000829	0.719170
-3.666044	-1.512766	3.881318	0.000746	0.719263
-3.563158	-1.529687	3.891315	0.000727	0.719267
-3.545420	-1.533742	3.901312	0.000723	0.719265
-2.985166	-1.476972	3.911309	0.000618	0.719575
-2.699951	-1.517324	3.921306	0.000565	0.719596
-2.841866	-1.491360	3.931302	0.000591	0.719598
-2.667491	-1.466847	3.941299	0.000558	0.719708
-2.194681	-1.456602	3.951296	0.000470	0.719895
-2.134806	-1.466694	3.961293	0.000459	0.719896
-2.084176	-1.459074	3.971290	0.000449	0.719930
-1.709493	-1.380135	3.981286	0.000379	0.720217
-1.405450	-1.433311	3.991283	0.000322	0.720220
-1.527337	-1.394445	4.001280	0.000344	0.720254
-1.579858	-1.241741	4.011277	0.000353	0.720537
-1.430091	-1.270460	4.021274	0.000325	0.720533
-1.201832	-1.201856	4.031270	0.000282	0.720749
-0.999033	-1.175320	4.041267	0.000244	0.720873
-0.918240	-1.149769	4.051264	0.000229	0.720952
-0.947430	-1.060288	4.061261	0.000234	0.721118
-0.828749	-1.045802	4.071258	0.000212	0.721189
-0.986063	-0.893251	4.081254	0.000240	0.721435
-1.044478	-0.816123	4.091251	0.000251	0.721566
-0.734895	-0.783116	4.101248	0.000193	0.721740
-0.580627	-0.686509	4.111245	0.000164	0.721985
-0.405431	-0.666803	4.121242	0.000131	0.722085
-0.299024	-0.544696	4.131238	0.000111	0.722363
-0.137924	-0.493549	4.141235	0.000080	0.722520
-0.689034	-0.297812	4.151232	0.000183	0.722712
-0.446418	-0.192425	4.161229	0.000137	0.723004
-0.015354	-0.146274	4.171226	0.000056	0.723246
-0.035752	-0.044934	4.181222	0.000060	0.723438
0.104173	0.035066	4.191219	0.000033	0.723644
0.000000	0.268106	4.201216	0.000052	0.724065

0.317505	0.850086	4.206221	-0.000007	0.725315
0.203844	2.123713	4.211226	0.000013	0.727762
0.322102	3.972315	4.216230	-0.000011	0.731397
0.765572	6.299058	4.221235	-0.000095	0.736047
1.011182	9.181099	4.226240	-0.000143	0.741663
1.277664	12.543486	4.231245	-0.000194	0.748156
1.612628	16.336089	4.236250	-0.000259	0.755423
2.233134	20.494083	4.241254	-0.000378	0.763394
2.520244	25.111050	4.246259	-0.000435	0.772017
2.817986	30.090490	4.251264	-0.000493	0.781207
3.455084	35.364025	4.256269	-0.000616	0.790925
3.718663	41.007897	4.261274	-0.000669	0.801064
4.038159	46.961534	4.266278	-0.000732	0.811634
4.547275	53.143355	4.271283	-0.000831	0.822520
5.079243	59.612651	4.276288	-0.000934	0.833759
5.507591	66.309814	4.281293	-0.001019	0.845200
5.990993	73.218888	4.286298	-0.001113	0.856855
6.659795	80.314626	4.291302	-0.001243	0.868711
7.162821	87.612527	4.296307	-0.001341	0.880686
7.481086	95.127595	4.301312	-0.001406	0.892793
8.362404	102.696592	4.306317	-0.001575	0.904977
9.134046	110.444184	4.311322	-0.001724	0.917246
9.593469	118.361360	4.316326	-0.001815	0.929527
10.425703	126.330968	4.321331	-0.001975	0.941825
11.238509	134.423108	4.326336	-0.002132	0.954141
11.714302	142.648143	4.331341	-0.002226	0.966408
12.372627	150.917738	4.336346	-0.002354	0.978632
13.003584	159.286368	4.341350	-0.002477	0.990839
13.524434	167.699082	4.346355	-0.002580	1.002933
14.085125	176.158308	4.351360	-0.002690	1.014957
15.265945	184.549726	4.356365	-0.002915	1.026895
16.858921	192.927154	4.361370	-0.003217	1.038773
17.544738	201.514692	4.366374	-0.003351	1.050588
17.993432	210.147770	4.371379	-0.003440	1.062277
18.583037	218.793024	4.376384	-0.003556	1.073887
19.719521	227.327119	4.381389	-0.003773	1.085350
20.172259	236.005348	4.386394	-0.003863	1.096727
20.839680	244.651454	4.391398	-0.003993	1.107993
21.380423	253.309393	4.396403	-0.004100	1.119132
21.743664	262.007169	4.401408	-0.004173	1.130173
22.713889	270.595068	4.406413	-0.004360	1.141100
23.232659	279.278001	4.411418	-0.004462	1.151945
23.739475	287.935033	4.416422	-0.004562	1.162654
24.257765	296.567289	4.421427	-0.004664	1.173238
25.288607	305.097890	4.426432	-0.004862	1.183709
25.913033	313.712156	4.431437	-0.004984	1.194106
26.137665	322.348219	4.436442	-0.005032	1.204357
26.910942	330.906972	4.441446	-0.005182	1.214541
27.369879	339.486710	4.446451	-0.005273	1.224603
27.971532	348.062821	4.451456	-0.005390	1.234605
29.067005	356.507393	4.456461	-0.005600	1.244473
29.463691	365.074248	4.461466	-0.005680	1.254266
29.923479	373.618875	4.466470	-0.005771	1.263971
30.610439	382.111803	4.471475	-0.005905	1.273587
31.203161	390.595271	4.476480	-0.006021	1.283102
31.838911	399.070366	4.481485	-0.006145	1.292546
32.414564	407.535520	4.486490	-0.006258	1.301899
32.926338	416.087757	4.491494	-0.006359	1.311268
33.318593	424.597603	4.496499	-0.006437	1.320503
33.911303	433.002338	4.501504	-0.006553	1.329598
34.268568	441.442626	4.506509	-0.006626	1.338626
34.834067	449.828611	4.511514	-0.006737	1.347573
35.390441	458.226382	4.516518	-0.006846	1.356472
36.063122	466.570045	4.521523	-0.006977	1.365276
36.340323	474.995021	4.526528	-0.007034	1.374040
36.505867	483.416262	4.531533	-0.007070	1.382725
36.771426	491.817035	4.536538	-0.007125	1.391352
37.795950	500.084900	4.541542	-0.007322	1.399918
38.280587	508.416050	4.546547	-0.007418	1.408406
38.645379	516.780146	4.551552	-0.007491	1.416856
38.982247	525.124663	4.556557	-0.007559	1.425231
39.529721	533.433382	4.561562	-0.007667	1.433556
40.187605	541.713643	4.566566	-0.007795	1.441823
40.761456	550.009601	4.571571	-0.007907	1.450045
41.223916	558.336961	4.576576	-0.007999	1.458232
41.924445	566.595025	4.581581	-0.008135	1.466344
42.166517	574.979580	4.586586	-0.008186	1.474461
42.657936	583.263233	4.591590	-0.008283	1.482476
43.140936	591.524184	4.596595	-0.008378	1.490425
43.590877	599.809255	4.601600	-0.008468	1.498349
44.006115	608.077618	4.606605	-0.008550	1.506210
44.846984	616.284197	4.611610	-0.008713	1.514037
45.285397	624.556631	4.616614	-0.008800	1.521824
45.725506	632.812114	4.621619	-0.008887	1.529555
46.165223	641.080573	4.626624	-0.008975	1.537260
46.584151	649.335932	4.631629	-0.009058	1.544911
46.882137	657.624327	4.636634	-0.009119	1.552536
47.627017	665.816432	4.641638	-0.009263	1.560102
48.018292	674.052676	4.646643	-0.009342	1.567619
48.241111	682.336559	4.651648	-0.009389	1.575119
48.640301	690.567814	4.656653	-0.009469	1.582562
48.980520	698.795974	4.661658	-0.009538	1.589958
49.474782	707.024227	4.666662	-0.009635	1.597342
49.610071	715.261649	4.671667	-0.009666	1.604649
50.299133	723.440544	4.676672	-0.009800	1.611949
50.833685	731.640528	4.681677	-0.009905	1.619214
51.227343	739.838514	4.686682	-0.009983	1.626424
51.553768	748.134892	4.691686	-0.010050	1.633678
52.115858	756.275064	4.696691	-0.010160	1.640797
52.499623	764.467335	4.701696	-0.010237	1.647906
52.839442	772.682567	4.706701	-0.010306	1.654998
53.046074	780.881360	4.711706	-0.010350	1.662028
53.546996	789.061963	4.716710	-0.010448	1.669052
53.952599	797.246363	4.721715	-0.010529	1.676037
54.378234	805.416579	4.726720	-0.010614	1.682983
54.765297	813.607777	4.731725	-0.010692	1.689913
55.136215	821.788848	4.736730	-0.010766	1.696805
55.618401	829.958446	4.741734	-0.010862	1.703673
56.443149	838.083619	4.746739	-0.011021	1.710521
56.686701	846.301749	4.751744	-0.011071	1.717343
57.022772	854.467987	4.756749	-0.011139	1.724108
57.358067	862.640663	4.761754	-0.011207	1.730851
57.793628	870.815502	4.766758	-0.011294	1.737582
58.036361	878.988886	4.771763	-0.011345	1.744261
58.429184	887.155157	4.776768	-0.011423	1.750928
58.908336	895.321481	4.781773	-0.011518	1.757581
59.049395	903.483328	4.786778	-0.011550	1.764162
59.554016	911.637136	4.791782	-0.011649	1.770758
59.854580	919.809551	4.796787	-0.011711	1.777318
60.323082	927.947845	4.801792	-0.011803	1.783848
60.644701	936.135503	4.806797	-0.011869	1.790375
60.977339	944.324341	4.811802	-0.011936	1.796881
61.599813	952.425968	4.816806	-0.012057	1.803329
61.785884	960.583008	4.821811	-0.012098	1.809745
62.210625	968.720532	4.826816	-0.012182	1.816152
62.711905	976.831818	4.831821	-0.012281	1.822525
63.266268	984.941441	4.836826	-0.012390	1.828881
63.545820	993.115830	4.841830	-0.012447	1.835232
63.867383	1001.244559	4.846835	-0.012512	1.841530
64.205742	1009.379924	4.851840	-0.012581	1.847814
64.608867	1017.536875	4.856845	-0.012661	1.854101
64.858545	1025.666841	4.861850	-0.012713	1.860328
65.334571	1033.794233	4.866854	-0.012807	1.866559
65.786063	1041.936882	4.871859	-0.012897	1.872777
65.983443	1050.094605	4.876864	-0.012939	1.878956
66.479032	1058.186800	4.881869	-0.013037	1.885101
66.850299	1066.312055	4.886874	-0.013112	1.891235
67.179516	1074.458303	4.891878	-0.013178	1.897361
67.364383	1082.585300	4.896883	-0.013218	1.903436
67.581224	1090.746243	4.901888	-0.013264	1.909521
67.832718	1098.894186	4.906893	-0.013316	1.915581
68.065578	1106.997254	4.911898	-0.013365	1.921586
68.476241	1115.102047	4.916902	-0.013447	1.927593
68.616871	1123.255286	4.921907	-0.013479	1.933587
68.972492	1131.354140	4.926912	-0.013550	1.939547
69.366695	1139.461065	4.931917	-0.013629	1.945498
69.811601	1147.580187	4.936922	-0.013717	1.951446
70.258384	1155.703697	4.941926	-0.013806	1.957378
70.664658	1163.771290	4.946931	-0.013887	1.963248
71.002074	1171.882375	4.951936	-0.013955	1.969124
71.136527	1180.034144	4.956941	-0.013986	1.974990
71.323142	1188.140690	4.961946	-0.014026	1.980812
71.860679	1196.222292	4.966950	-0.014132	1.986636
72.165661	1204.337178	4.971955	-0.014194	1.992442
72.530715	1212.444831	4.976960	-0.014267	1.998232
72.784126	1220.550452	4.981965	-0.014320	2.003992
73.191425	1228.633780	4.986970	-0.014401	2.009736
73.538539	1236.767940	4.991974	-0.014471	2.015493
73.703474	1244.878351	4.996979	-0.014507	2.021198
74.014077	1252.987434	5.001984	-0.014571	2.026901
74.256672	1261.136823	5.006989	-0.014621	2.032609
74.568527	1269.217321	5.011994	-0.014685	2.038260
74.902681	1277.296727	5.016998	-0.014752	2.043897
75.311119	1285.383980	5.022003	-0.014834	2.049532
75.606443	1293.487066	5.027008	-0.014894	2.055150
76.242113	1301.536630	5.032013	-0.015018	2.060750
76.731136	1309.598143	5.037018	-0.015115	2.066328
76.797328	1317.780127	5.042022	-0.015132	2.071932
76.941818	1325.891578	5.047027	-0.015165	2.077480
77.206431	1333.968532	5.052032	-0.015219	2.083001
77.684295	1342.051804	5.057037	-0.015314	2.088534
77.848678	1350.162916	5.062042	-0.015350	2.094039
78.127476	1358.260870	5.067046	-0.015407	2.099532
78.689151	1366.309824	5.072051	-0.015517	2.105006
79.052832	1374.433714	5.077056	-0.015590	2.110496
79.469487	1382.576077	5.082061	-0.015673	2.115989
79.783593	1390.619710	5.087066	-0.015737	2.121393
80.103568	1398.708363	5.092070	-0.015802	2.126813
80.339521	1406.809060	5.097075	-0.015852	2.132219
80.546512	1414.909915	5.102080	-0.015896	2.137608
80.771825	1422.994959	5.107085	-0.015943	2.142976
80.763603	1431.114710	5.112090	-0.015947	2.148330
81.106865	1439.211588	5.117094	-0.016016	2.153690
81.533328	1447.257488	5.122099	-0.016101	2.159010
81.621031	1455.337984	5.127104	-0.016123	2.164308
82.010541	1463.421222	5.132109	-0.016201	2.169623
82.287664	1471.503625	5.137114	-0.016258	2.174914
82.684977	1479.573469	5.142118	-0.016337	2.180195
82.907797	1487.657803	5.147123	-0.016384	2.185457
83.192042	1495.761798	5.152128	-0.016443	2.190724
83.405665	1503.881945	5.157133	-0.016488	2.195982
83.819540	1511.912824	5.162138	-0.016570	2.201189
84.189860	1519.984999	5.167142	-0.016645	2.206406
84.334056	1528.085236	5.172147	-0.016677	2.211608
84.686631	1536.156033	5.177152	-0.016748	2.216797
84.865079	1544.253069	5.182157	-0.016787	2.221976
85.248586	1552.300078	5.187162	-0.016863	2.227128
85.477236	1560.414304	5.192166	-0.016911	2.232298
85.832324	1568.480217	5.197171	-0.016983	2.237437
86.187140	1576.522673	5.202176	-0.017054	2.242548
86.306195	1584.646389	5.207181	-0.017082	2.247679
86.543615	1592.732262	5.212186	-0.017132	2.252784
87.087189	1600.776888	5.217190	-0.017238	2.257878
87.501507	1608.834566	5.222195	-0.017321	2.262958
87.782873	1616.909831	5.227200	-0.017379	2.268026
87.945854	1625.088481	5.232205	-0.017415	2.273136
88.419086	1633.095465	5.237210	-0.017508	2.278156
88.681282	1641.157406	5.242214	-0.017562	2.283179
88.817333	1649.226928	5.247219	-0.017593	2.288186
88.959667	1657.321716	5.252224	-0.017625	2.293198
89.485820	1665.356943	5.257229	-0.017728	2.298195
89.482373	1673.442871	5.262234	-0.017733	2.303167
89.922409	1681.499216	5.267238	-0.017820	2.308148
90.196828	1689.590600	5.272243	-0.017877	2.313125
90.731340	1697.604710	5.277248	-0.017982	2.318066
90.861255	1705.703848	5.282253	-0.018012	2.323015
91.181240	1713.753858	5.287258	-0.018077	2.327939
91.725318	1721.823063	5.292262	-0.018183	2.332883
91.868590	1729.911900	5.297267	-0.018215	2.337795
92.126171	1737.977006	5.302272	-0.018269	2.342692
92.637401	1746.027895	5.307277	-0.018369	2.347590
92.656606	1754.151922	5.312282	-0.018378	2.352482
92.898522	1762.237029	5.317286	-0.018429	2.357359
93.025886	1770.292220	5.322291	-0.018458	2.362198
93.323242	1778.338501	5.327296	-0.018519	2.367036
93.327728	1786.448201	5.332301	-0.018525	2.371879
93.960522	1794.451493	5.337306	-0.018648	2.376698
94.220531	1802.516760	5.342310	-0.018702	2.381514
94.314625	1810.608924	5.347315	-0.018725	2.386324
94.614838	1818.664312	5.352320	-0.018786	2.391118
94.933661	1826.732004	5.357325	-0.018851	2.395911
95.059821	1834.786677	5.362330	-0.018880	2.400672
95.375427	1842.849183	5.367334	-0.018944	2.405443
95.584228	1850.917388	5.372339	-0.018988	2.410200
95.967929	1858.980311	5.377344	-0.019065	2.414957
96.183666	1867.063518	5.382349	-0.019111	2.419704
96.471214	1875.097856	5.387354	-0.019170	2.424418
96.702850	1883.174459	5.392358	-0.019218	2.429144
96.958947	1891.317440	5.397363	-0.019272	2.433901
97.138403	1899.354767	5.402368	-0.019310	2.438581
97.544095	1907.384347	5.407373	-0.019391	2.443265
97.645931	1915.431462	5.412378	-0.019416	2.447927
98.145452	1923.483745	5.417382	-0.019514	2.452614
98.254459	1931.559015	5.422387	-0.019540	2.457275
98.400320	1939.591349	5.427392	-0.019572	2.461905
98.743143	1947.652640	5.432397	-0.019642	2.466558
98.955312	1955.715067	5.437402	-0.019686	2.471193
99.350136	1963.786466	5.442406	-0.019765	2.475838
99.463149	1971.845614	5.447411	-0.019792	2.480446
99.543785	1979.894143	5.452416	-0.019812	2.485037
99.787050	1987.971970	5.457421	-0.019863	2.489648
100.078448	1996.015760	5.462426	-0.019923	2.494235
100.355959	2004.082690	5.467430	-0.019980	2.498826
100.872275	2012.080205	5.472435	-0.020081	2.503386
100.973037	2020.168354	5.477440	-0.020105	2.507959
101.233854	2028.283736	5.482445	-0.020159	2.512551
101.577008	2036.301040	5.487450	-0.020229	2.517084
102.105471	2044.319816	5.492454	-0.020332	2.521624
102.482893	2052.350152	5.497459	-0.020408	2.526151
102.852737	2060.412309	5.502464	-0.020482	2.530687
103.126012	2068.488355	5.507469	-0.020539	2.535216
103.194766	2076.552127	5.512474	-0.020557	2.539715
103.335311	2084.623074	5.517478	-0.020589	2.544216
103.488150	2092.692216	5.522483	-0.020622	2.548708
103.957862	2100.728139	5.527488	-0.020715	2.553196
104.158603	2108.793684	5.532493	-0.020758	2.557674
104.341187	2116.814990	5.537498	-0.020797	2.562118
104.713265	2124.877106	5.542502	-0.020872	2.566590
104.932823	2132.948362	5.547507	-0.020918	2.571049
104.821789	2141.054101	5.552512	-0.020903	2.575496
105.114333	2149.090560	5.557517	-0.020963	2.579925
105.495239	2157.087127	5.562522	-0.021039	2.584331
105.742474	2165.172066	5.567526	-0.021091	2.588768
106.222824	2173.361219	5.572531	-0.021186	2.593270
106.441387	2181.389165	5.577536	-0.021232	2.597659
106.818256	2189.379186	5.582541	-0.021307	2.602031
107.110340	2197.386253	5.587546	-0.021367	2.606399
107.470982	2205.416561	5.592550	-0.021440	2.610776
107.517865	2213.512831	5.597555	-0.021454	2.615161
107.902226	2221.499321	5.602560	-0.021531	2.619501
108.313001	2229.543817	5.607565	-0.021613	2.623868
108.355360	2237.611254	5.612570	-0.021626	2.628215
108.533597	2245.701464	5.617574	-0.021665	2.632576
108.847551	2253.736078	5.622579	-0.021728	2.636909
109.258398	2261.733982	5.627584	-0.021810	2.641221
109.345582	2269.809217	5.632589	-0.021832	2.645546
109.456647	2277.861450	5.637594	-0.021858	2.649854
109.882616	2285.921404	5.642598	-0.021943	2.654179
109.935182	2293.995814	5.647603	-0.021958	2.658481
109.900204	2302.037000	5.652608	-0.021957	2.662752
110.167011	2310.091400	5.657613	-0.022012	2.667043
110.608093	2318.144807	5.662618	-0.022100	2.671337
110.920229	2326.212340	5.667622	-0.022163	2.675624
111.550010	2334.200625	5.672627	-0.022286	2.679883
111.761250	2342.228973	5.677632	-0.022330	2.684129
112.088059	2350.269844	5.682637	-0.022397	2.688382
112.004735	2358.362456	5.687642	-0.022387	2.692629
112.259255	2366.413393	5.692646	-0.022439	2.696870
112.733344	2374.411372	5.697651	-0.022533	2.701089
112.847879	2382.452790	5.702656	-0.022560	2.705302
112.930039	2390.537625	5.707661	-0.022580	2.709530
113.291098	2398.575980	5.712666	-0.022653	2.713743
113.332389	2406.641865	5.717670	-0.022666	2.717945
113.462613	2414.669376	5.722675	-0.022696	2.722126
113.861208	2422.683353	5.727680	-0.022775	2.726309
114.156771	2430.748062	5.732685	-0.022836	2.730507
114.358643	2438.806895	5.737690	-0.022879	2.734689
114.839385	2446.839075	5.742694	-0.022974	2.738867
115.083446	2454.865180	5.747699	-0.023025	2.743022
115.023651	2462.934657	5.752704	-0.023019	2.747174
115.162492	2471.063970	5.757709	-0.023050	2.751363
115.524635	2479.125908	5.762714	-0.023123	2.755524
115.771990	2487.131473	5.767718	-0.023174	2.759644
115.796383	2495.160064	5.772723	-0.023184	2.763755
116.199887	2503.159867	5.777728	-0.023265	2.767868
116.584023	2511.221821	5.782733	-0.023342	2.772006
116.800768	2519.253065	5.787738	-0.023388	2.776112
116.962625	2527.295976	5.792742	-0.023423	2.780214
117.317434	2535.301346	5.797747	-0.023495	2.784302
117.534346	2543.355656	5.802752	-0.023540	2.788402
117.890342	2551.437263	5.807757	-0.023612	2.792517
118.504662	2559.415226	5.812762	-0.023732	2.796588
118.925111	2567.446761	5.817766	-0.023815	2.800670
118.947945	2575.505187	5.822771	-0.023825	2.804736
119.388864	2583.519077	5.827776	-0.023913	2.808797
119.791689	2591.597042	5.832781	-0.023993	2.812883
119.859611	2599.655148	5.837786	-0.024011	2.816934
120.156619	2607.696138	5.842790	-0.024072	2.820983
120.450230	2615.738636	5.847795	-0.024132	2.825027
120.501123	2623.804320	5.852800	-0.024147	2.829063
120.614385	2631.906355	5.857805	-0.024173	2.833114
120.736484	2639.927565	5.862810	-0.024201	2.837121
121.259265	2647.932206	5.867814	-0.024304	2.841135
121.170855	2655.977613	5.872819	-0.024293	2.845130
121.574014	2663.989921	5.877824	-0.024374	2.849131
121.923650	2672.080902	5.882829	-0.024444	2.853162
121.954858	2680.104623	5.887834	-0.024455	2.857136
122.148781	2688.155325	5.892838	-0.024497	2.861127
122.434369	2696.150745	5.897843	-0.024555	2.865090
122.551770	2704.211779	5.902848	-0.024583	2.869070
122.736659	2712.294916	5.907853	-0.024622	2.873060
122.835356	2720.310714	5.912858	-0.024646	2.877006
123.134613	2728.356532	5.917862	-0.024707	2.880972
123.314670	2736.364456	5.922867	-0.024746	2.884908
123.715955	2744.373464	5.927872	-0.024826	2.888851
124.025998	2752.462569	5.932877	-0.024889	2.892823
124.108325	2760.506972	5.937882	-0.024910	2.896755
124.571859	2768.530387	5.942886	-0.025002	2.900693
124.768640	2776.561733	5.947891	-0.025044	2.904614
124.772774	2784.633661	5.952896	-0.025050	2.908539
125.031510	2792.737348	5.957901	-0.025104	2.912488
125.388408	2800.751838	5.962906	-0.025176	2.916394
125.793475	2808.731987	5.967910	-0.025256	2.920280
125.933286	2816.752707	5.972915	-0.025288	2.924167
126.021286	2824.793082	5.977920	-0.025310	2.928055
126.343709	2832.848394	5.982925	-0.025375	2.931957
126.609656	2840.886402	5.987930	-0.025430	2.935843
126.595967	2848.934467	5.992934	-0.025433	2.939714
126.911142	2856.953517	5.997939	-0.025497	2.943583
127.221179	2864.958458	6.002944	-0.025560	2.947440
127.513641	2873.029421	6.007949	-0.025620	2.951323
127.691175	2881.084422	6.012954	-0.025658	2.955187
127.739769	2889.122135	6.017958	-0.025673	2.959030
127.871886	2897.170506	6.022963	-0.025703	2.962879
127.938312	2905.165693	6.027968	-0.025720	2.966693
128.533735	2913.202413	6.032973	-0.025837	2.970549
128.432977	2921.279749	6.037978	-0.025823	2.974384
128.602506	2929.297788	6.042982	-0.025860	2.978200
129.012408	2937.322307	6.047987	-0.025942	2.982026
129.168280	2945.338887	6.052992	-0.025976	2.985831
129.415135	2953.404988	6.057997	-0.026028	2.989658
129.453221	2961.495775	6.063002	-0.026040	2.993482
129.746200	2969.512998	6.068006	-0.026100	2.997279
130.185307	2977.501896	6.073011	-0.026187	3.001065
130.154665	2985.505536	6.078016	-0.026187	3.004830
130.573977	2993.543611	6.083021	-0.026271	3.008628
130.765059	3001.594097	6.088026	-0.026312	3.012417
130.925399	3009.670046	6.093030	-0.026347	3.016210
131.093389	3017.697404	6.098035	-0.026383	3.019977
131.338486	3025.689408	6.103040	-0.026434	3.023726
131.672143	3033.742427	6.108045	-0.026502	3.027504
131.898247	3041.794114	6.113050	-0.026550	3.031270
131.976736	3049.875979	6.118054	-0.026570	3.035039
132.325735	3057.864677	6.123059	-0.026640	3.038773
132.280071	3065.897534	6.128064	-0.026637	3.042504
132.426196	3073.955411	6.133069	-0.026669	3.046251
132.618947	3081.963224	6.138074	-0.026711	3.049972
132.758715	3090.029561	6.143078	-0.026742	3.053714
133.036187	3098.049835	6.148083	-0.026799	3.057436
133.432806	3106.055636	6.153088	-0.026878	3.061152
133.714252	3114.096714	6.158093	-0.026936	3.064875
134.215506	3122.114412	6.163098	-0.027035	3.068593
134.730116	3130.212017	6.168102	-0.027136	3.072343
135.104224	3138.287194	6.173107	-0.027211	3.076072
135.203079	3146.254024	6.178112	-0.027235	3.079734
135.296622	3154.293613	6.183117	-0.027258	3.083424
135.613996	3162.316826	6.188122	-0.027322	3.087113
135.771911	3170.352253	6.193126	-0.027357	3.090796
136.124270	3178.391424	6.198131	-0.027428	3.094485
136.381674	3186.373940	6.203136	-0.027481	3.098139
136.693940	3194.426994	6.208141	-0.027545	3.101824
136.745421	3202.444561	6.213146	-0.027560	3.105476
136.942634	3210.487251	6.218150	-0.027602	3.109142
137.237122	3218.548401	6.223155	-0.027662	3.112816
137.114110	3226.602988	6.228160	-0.027645	3.116464
137.569137	3234.601885	6.233165	-0.027735	3.120109
137.544248	3242.631087	6.238170	-0.027736	3.123741
137.806797	3250.655668	6.243174	-0.027790	3.127380
138.266503	3258.687540	6.248179	-0.027881	3.131027
138.381124	3266.745751	6.253184	-0.027908	3.134666
138.506408	3274.799857	6.258189	-0.027936	3.138300
138.793031	3282.787798	6.263194	-0.027995	3.141906
139.011644	3290.827887	6.268198	-0.028041	3.145529
139.359753	3298.842415	6.273203	-0.028111	3.149142
139.438828	3306.917696	6.278208	-0.028132	3.152766
139.639580	3314.978594	6.283213	-0.028174	3.156384
140.106769	3322.960772	6.288218	-0.028267	3.159975
140.277128	3330.969911	6.293222	-0.028304	3.163561
140.622940	3339.011821	6.298227	-0.028374	3.167165
140.683030	3347.047262	6.303232	-0.028390	3.170750
141.316465	3355.084195	6.308237	-0.028514	3.174356
141.515555	3363.095877	6.313242	-0.028556	3.177928
141.609698	3371.151379	6.318246	-0.028579	3.181511
142.000881	3379.157248	6.323251	-0.028657	3.185080
141.985946	3387.228098	6.328256	-0.028660	3.188657
142.305777	3395.283078	6.333261	-0.028725	3.192237
142.532262	3403.308139	6.338266	-0.028772	3.195796
142.745978	3411.325095	6.343270	-0.028817	3.199346
142.897380	3419.346370	6.348275	-0.028851	3.202892
143.248661	3427.352713	6.353280	-0.028922	3.206436
143.457772	3435.409210	6.358285	-0.028966	3.209992
143.502101	3443.445558	6.363290	-0.028980	3.213528
143.585009	3451.499953	6.368294	-0.029001	3.217070
143.956137	3459.513402	6.373299	-0.029075	3.220602
144.269208	3467.478575	6.378304	-0.029139	3.224107
144.519552	3475.543340	6.383309	-0.029191	3.227648
144.784210	3483.624328	6.388314	-0.029246	3.231193
145.041056	3491.691464	6.393318	-0.029299	3.234729
145.019765	3499.703245	6.398323	-0.029300	3.238224
145.379333	3507.666116	6.403328	-0.029372	3.241710
145.915100	3515.662305	6.408333	-0.029478	3.245214
145.681454	3523.731347	6.413338	-0.029440	3.248715
145.919164	3531.775570	6.418342	-0.029489	3.252220
146.476370	3539.817899	6.423347	-0.029598	3.255733
146.472563	3547.811941	6.428352	-0.029603	3.259199
146.502301	3555.881378	6.433357	-0.029614	3.262695
146.973223	3563.867161	6.438362	-0.029707	3.266169
147.232422	3571.898350	6.443366	-0.029761	3.269651
147.250674	3579.989841	6.448371	-0.029769	3.273145
147.419136	3587.994500	6.453376	-0.029806	3.276604
147.636926	3596.000333	6.458381	-0.029852	3.280061
147.979651	3603.996162	6.463386	-0.029921	3.283516
148.187578	3612.035282	6.468390	-0.029965	3.286980
148.334682	3620.094289	6.473395	-0.029998	3.290447
148.276025	3628.145422	6.478400	-0.029993	3.293898
148.641462	3636.179327	6.483405	-0.030066	3.297355
148.864102	3644.191578	6.488410	-0.030113	3.300794
149.120326	3652.182275	6.493414	-0.030166	3.304221
149.412332	3660.230123	6.498419	-0.030226	3.307670
149.612819	3668.258060	6.503424	-0.030269	3.311104
149.790902	3676.339654	6.508429	-0.030307	3.314556
149.925141	3684.328026	6.513434	-0.030337	3.317963
150.076184	3692.343021	6.518438	-0.030371	3.321378
150.308398	3700.340815	6.523443	-0.030420	3.324786
150.568373	3708.367300	6.528448	-0.030473	3.328203
150.728038	3716.460317	6.533453	-0.030509	3.331641
150.778033	3724.509450	6.538458	-0.030523	3.335053
150.887253	3732.493784	6.543462	-0.030549	3.338437
151.112620	3740.524173	6.548467	-0.030596	3.341840
151.503886	3748.495186	6.553472	-0.030675	3.345221
151.678238	3756.594704	6.558477	-0.030712	3.348645
151.854341	3764.624640	6.563482	-0.030751	3.352037
151.990636	3772.691460	6.568486	-0.030781	3.355438
152.286988	3780.695564	6.573491	-0.030842	3.358816
152.442063	3788.677655	6.578496	-0.030876	3.362176
152.661882	3796.702435	6.583501	-0.030923	3.365553
152.886820	3804.739417	6.588506	-0.030970	3.368931
152.992373	3812.798507	6.593510	-0.030995	3.372311
153.380913	3820.866998	6.598515	-0.031073	3.375702
153.396668	3828.833550	6.603520	-0.031081	3.379034
153.811942	3836.861577	6.608525	-0.031164	3.382402
153.896274	3844.890640	6.613530	-0.031185	3.385755
153.961580	3852.906838	6.618534	-0.031202	3.389099
154.329125	3861.015784	6.623539	-0.031276	3.392489
154.454553	3869.070035	6.628544	-0.031305	3.395844
154.519130	3877.047237	6.633549	-0.031322	3.399162
154.571200	3885.053629	6.638554	-0.031337	3.402488
154.963344	3893.035733	6.643558	-0.031416	3.405813
155.018111	3901.065233	6.648563	-0.031431	3.409142
155.089107	3909.105793	6.653568	-0.031450	3.412473
155.433773	3917.157243	6.658573	-0.031520	3.415815
155.650059	3925.139672	6.663578	-0.031565	3.419121
155.853728	3933.152919	6.668582	-0.031608	3.422435
155.983311	3941.195285	6.673587	-0.031638	3.425756
156.155728	3949.207887	6.678592	-0.031675	3.429063
156.245838	3957.304116	6.683597	-0.031698	3.432398
156.504042	3965.323884	6.688602	-0.031751	3.435704
156.761034	3973.308262	6.693606	-0.031804	3.438993
156.739982	3981.367930	6.698611	-0.031806	3.442300
156.826347	3989.370252	6.703616	-0.031827	3.445583
157.148457	3997.409979	6.708621	-0.031893	3.448887
157.264472	4005.466582	6.713626	-0.031920	3.452188
157.445583	4013.502791	6.718630	-0.031959	3.455479
157.709117	4021.504185	6.723635	-0.032013	3.458755
157.969705	4029.516595	6.728640	-0.032067	3.462033
158.175842	4037.539548	6.733645	-0.032111	3.465310
158.242189	4045.609730	6.738650	-0.032129	3.468599
158.590099	4053.621443	6.743654	-0.032199	3.471870
158.813050	4061.690759	6.748659	-0.032246	3.475157
158.886609	4069.680435	6.753664	-0.032265	3.478404
159.309128	4077.685465	6.758669	-0.032349	3.481665
159.457546	4085.653531	6.763674	-0.032382	3.484900
159.406110	4093.692607	6.768678	-0.032378	3.488153
159.590283	4101.763162	6.773683	-0.032417	3.491424
159.937616	4109.755974	6.778688	-0.032487	3.494666
160.281127	4117.796895	6.783693	-0.032557	3.497924
160.456593	4125.843848	6.788698	-0.032595	3.501176
160.608848	4133.800978	6.793702	-0.032629	3.504387
160.879332	4141.841654	6.798707	-0.032684	3.507634
161.125162	4149.882498	6.803712	-0.032735	3.510876
161.489710	4157.900767	6.808717	-0.032809	3.514110
161.873788	4165.915764	6.813722	-0.032886	3.517341
161.966498	4173.946634	6.818726	-0.032908	3.520565
162.365419	4181.945918	6.823731	-0.032988	3.523784
162.639629	4189.984838	6.828736	-0.033044	3.527011
162.867280	4198.013718	6.833741	-0.033092	3.530230
162.947065	4206.069853	6.838746	-0.033112	3.533453
163.417763	4214.074862	6.843750	-0.033205	3.536664
163.553295	4222.150248	6.848755	-0.033236	3.539890
163.516125	4230.140290	6.853760	-0.033235	3.543074
163.914742	4238.185564	6.858765	-0.033314	3.546290
164.123722	4246.189735	6.863770	-0.033358	3.549481
164.169184	4254.324999	6.868774	-0.033372	3.552716
164.441656	4262.377655	6.873779	-0.033429	3.555922
164.644102	4270.294932	6.878784	-0.033472	3.559070
164.827216	4278.338925	6.883789	-0.033511	3.562264
165.028416	4286.320289	6.888794	-0.033554	3.565432
165.145622	4294.343455	6.893798	-0.033581	3.568610
165.468145	4302.377694	6.898803	-0.033647	3.571796
165.422067	4310.394113	6.903808	-0.033643	3.574962
165.508634	4318.439574	6.908813	-0.033665	3.578139
165.640949	4326.446125	6.913818	-0.033695	3.581300
165.670325	4334.450659	6.918822	-0.033706	3.584455
165.865931	4342.503364	6.923827	-0.033748	3.587630
166.242052	4350.493849	6.928832	-0.033823	3.590784
166.534501	4358.561166	6.933837	-0.033883	3.593962
166.925337	4366.542756	6.938842	-0.033961	3.597106
167.108161	4374.560782	6.943846	-0.034000	3.600256
167.332279	4382.566226	6.948851	-0.034047	3.603400
167.628759	4390.582377	6.953856	-0.034108	3.606547
167.712487	4398.623216	6.958861	-0.034129	3.609695
167.819555	4406.668662	6.963866	-0.034154	3.612842
167.974990	4414.731352	6.968870	-0.034189	3.615995
168.008065	4422.741755	6.973875	-0.034200	3.619122
168.151048	4430.761781	6.978880	-0.034232	3.622252
168.561426	4438.751595	6.983885	-0.034314	3.625375
168.700660	4446.783532	6.988890	-0.034345	3.628505
168.905320	4454.835576	6.993894	-0.034389	3.631641
169.198670	4462.899760	6.998899	-0.034449	3.634782
169.249677	4470.876842	7.003904	-0.034464	3.637880
169.653617	4478.909600	7.008909	-0.034544	3.641006
169.946604	4486.875699	7.013914	-0.034604	3.644100
170.036152	4494.960336	7.018918	-0.034626	3.647233
169.976169	4503.004911	7.023923	-0.034621	3.650343
170.144676	4511.004313	7.028928	-0.034657	3.653439
170.570565	4519.056908	7.033933	-0.034742	3.656559
170.536095	4527.058066	7.038938	-0.034741	3.659646
170.581704	4535.072687	7.043942	-0.034755	3.662736
171.034413	4543.090061	7.048947	-0.034845	3.665836
171.137006	4551.126704	7.053952	-0.034869	3.668932
171.293617	4559.190107	7.058957	-0.034904	3.672036
171.664957	4567.184213	7.063962	-0.034978	3.675117
171.990368	4575.167933	7.068966	-0.035044	3.678190
172.189632	4583.238561	7.073971	-0.035087	3.681290
172.272566	4591.173046	7.078976	-0.035107	3.684333
172.599083	4599.256226	7.083981	-0.035174	3.687436
172.598740	4607.282263	7.088986	-0.035179	3.690507
172.792383	4615.319358	7.093990	-0.035220	3.693584
173.010848	4623.360800	7.098995	-0.035266	3.696661
173.159795	4631.285922	7.104000	-0.035300	3.699689
173.348208	4639.342816	7.109005	-0.035340	3.702765
173.728911	4647.367736	7.114010	-0.035416	3.705832
173.797908	4655.429579	7.119014	-0.035435	3.708903
173.952006	4663.500020	7.124019	-0.035469	3.711976
174.105459	4671.518913	7.129024	-0.035503	3.715027
174.509405	4679.516007	7.134029	-0.035583	3.718074
174.670835	4687.538706	7.139034	-0.035619	3.721121
174.656592	4695.468076	7.144038	-0.035621	3.724127
174.952203	4703.541577	7.149043	-0.035682	3.727192
175.090661	4711.544381	7.154048	-0.035713	3.730224
175.255075	4719.586809	7.159053	-0.035749	3.733269
175.526025	4727.617575	7.164058	-0.035805	3.736310
175.708677	4735.580328	7.169062	-0.035844	3.739321
176.224830	4743.648687	7.174067	-0.035946	3.742376
176.017483	4751.651525	7.179072	-0.035912	3.745388
176.291644	4759.689535	7.184077	-0.035969	3.748422
176.492474	4767.742900	7.189082	-0.036012	3.751457
176.569496	4775.757402	7.194086	-0.036031	3.754472
176.851787	4783.781487	7.199091	-0.036089	3.757493
176.957926	4791.793071	7.204096	-0.036115	3.760503
177.064181	4799.831104	7.209101	-0.036140	3.763521
177.355635	4807.838462	7.214106	-0.036199	3.766528
177.439141	4815.864221	7.219110	-0.036220	3.769536
177.649779	4823.911231	7.224115	-0.036265	3.772552
177.667514	4831.940566	7.229120	-0.036274	3.775554
177.885434	4839.954166	7.234125	-0.036320	3.778553
177.980841	4847.966561	7.239130	-0.036343	3.781546
177.982761	4855.959990	7.244134	-0.036348	3.784527
178.288559	4864.011919	7.249139	-0.036411	3.787535
178.644134	4872.038064	7.254144	-0.036482	3.790532
178.862453	4880.079731	7.259149	-0.036528	3.793529
178.967504	4888.095100	7.264154	-0.036553	3.796511
179.151485	4896.070963	7.269158	-0.036593	3.799479
179.360245	4904.126569	7.274163	-0.036637	3.802473
179.346170	4912.120038	7.279168	-0.036640	3.805438
179.688485	4920.128370	7.284173	-0.036709	3.808414
179.845541	4928.173328	7.289178	-0.036744	3.811396
179.982313	4936.149040	7.294182	-0.036775	3.814351
180.074375	4944.218904	7.299187	-0.036797	3.817337
180.146755	4952.215966	7.304192	-0.036816	3.820293
180.443649	4960.241019	7.309197	-0.036877	3.823262
180.522019	4968.278213	7.314202	-0.036897	3.826228
180.837153	4976.253071	7.319206	-0.036961	3.829175
181.194878	4984.342024	7.324211	-0.037033	3.832162
181.195313	4992.344026	7.329216	-0.037038	3.835107
181.311397	5000.366024	7.334221	-0.037065	3.838059
181.784507	5008.363068	7.339226	-0.037159	3.841007
181.941688	5016.364664	7.344230	-0.037193	3.843949
182.080058	5024.422892	7.349235	-0.037224	3.846908
182.369818	5032.401416	7.354240	-0.037284	3.849839
182.455456	5040.469123	7.359245	-0.037305	3.852796
182.402160	5048.526885	7.364250	-0.037301	3.855745
182.701379	5056.471422	7.369254	-0.037362	3.858656
182.979768	5064.540314	7.374259	-0.037419	3.861611
183.005867	5072.526728	7.379264	-0.037429	3.864528
183.283832	5080.600429	7.384269	-0.037486	3.867480
183.600832	5088.607210	7.389274	-0.037551	3.870406
183.721918	5096.820259	7.394278	-0.037579	3.873401
183.979256	5104.855646	7.399283	-0.037632	3.876332
184.444402	5112.695456	7.404288	-0.037724	3.879193
184.575470	5120.732732	7.409293	-0.037754	3.882117
184.606822	5128.715263	7.414298	-0.037765	3.885018
184.829724	5136.712502	7.419302	-0.037812	3.887925
185.119158	5144.724353	7.424307	-0.037871	3.890836
185.286253	5152.790170	7.429312	-0.037908	3.893763
185.511803	5160.813349	7.434317	-0.037955	3.896673
185.672514	5168.779582	7.439322	-0.037990	3.899559
185.660568	5176.827327	7.444326	-0.037993	3.902469
185.875334	5184.862350	7.449331	-0.038039	3.905377
185.998982	5192.845051	7.454336	-0.038067	3.908261
186.195230	5200.905260	7.459341	-0.038109	3.911173
186.291200	5208.966342	7.464346	-0.038132	3.914081
186.538149	5216.945962	7.469350	-0.038184	3.916961
187.025359	5224.922748	7.474355	-0.038280	3.919841
187.020131	5232.941126	7.479360	-0.038284	3.922726
187.319350	5240.960384	7.484365	-0.038345	3.925614
187.699693	5248.983320	7.489370	-0.038422	3.928503
187.726603	5257.033613	7.494374	-0.038432	3.931393
187.871188	5265.090041	7.499379	-0.038464	3.934285
188.122907	5273.065200	7.504384	-0.038517	3.937148
188.356634	5281.049791	7.509389	-0.038565	3.940012
188.312485	5289.091601	7.514394	-0.038563	3.942889
188.575162	5297.068227	7.519398	-0.038617	3.945746
189.021522	5305.136979	7.524403	-0.038705	3.948638
188.898967	5313.184621	7.529408	-0.038688	3.951509
189.023638	5321.241760	7.534413	-0.038717	3.954386
189.302380	5329.239531	7.539418	-0.038774	3.957243
189.527065	5337.187973	7.544422	-0.038821	3.960079
189.828152	5345.223614	7.549427	-0.038882	3.962945
189.881538	5353.206005	7.554432	-0.038898	3.965786
190.229403	5361.241553	7.559437	-0.038968	3.968649
190.357265	5369.304088	7.564442	-0.038997	3.971516
190.482276	5377.297871	7.569446	-0.039026	3.974356
190.643458	5385.365270	7.574451	-0.039061	3.977221
190.663215	5393.359762	7.579456	-0.039070	3.980055
190.913070	5401.380923	7.584461	-0.039122	3.982901
191.071902	5409.378658	7.589466	-0.039157	3.985735
191.147474	5417.425757	7.594470	-0.039177	3.988583
191.154137	5425.474768	7.599475	-0.039183	3.991428
191.330189	5433.470447	7.604480	-0.039221	3.994255
191.529457	5441.506199	7.609485	-0.039264	3.997095
191.743953	5449.509874	7.614490	-0.039309	3.999922
191.558827	5457.533948	7.619494	-0.039280	4.002747
191.935543	5465.545259	7.624499	-0.039356	4.005575
192.050717	5473.550240	7.629504	-0.039382	4.008395
192.173240	5481.611194	7.634509	-0.039411	4.011232
192.288080	5489.688921	7.639514	-0.039438	4.014073
192.292047	5497.681333	7.644518	-0.039444	4.016880
192.544650	5505.662094	7.649523	-0.039496	4.019685
192.541426	5513.658054	7.654528	-0.039501	4.022490
192.820169	5521.707801	7.659533	-0.039558	4.025315
193.125790	5529.746995	7.664538	-0.039620	4.028136
193.257669	5537.743311	7.669542	-0.039650	4.030937
193.471263	5545.896187	7.674547	-0.039696	4.033791
193.674324	5553.862380	7.679552	-0.039739	4.036579
193.787718	5561.803150	7.684557	-0.039765	4.039354
193.905971	5569.837815	7.689562	-0.039793	4.042160
194.151363	5577.783162	7.694566	-0.039844	4.044935
194.354054	5585.832658	7.699571	-0.039887	4.047743
194.238212	5593.844787	7.704576	-0.039871	4.050532
194.477503	5601.882477	7.709581	-0.039921	4.053333
194.708004	5609.927998	7.714586	-0.039969	4.056135
194.809133	5617.877641	7.719590	-0.039993	4.058899
195.076743	5625.957138	7.724595	-0.040048	4.061710
195.137790	5633.902398	7.729600	-0.040065	4.064468
195.196375	5641.967541	7.734605	-0.040081	4.067266
195.260287	5649.955159	7.739610	-0.040099	4.070036
195.458169	5658.008627	7.744614	-0.040141	4.072828
195.801059	5666.047413	7.749619	-0.040210	4.075616
195.682407	5674.016527	7.754624	-0.040193	4.078370
195.899419	5682.072411	7.759629	-0.040239	4.081158
196.186980	5690.028019	7.764634	-0.040298	4.083910
196.271746	5698.086733	7.769638	-0.040319	4.086693
196.654761	5706.102092	7.774643	-0.040396	4.089463
196.663761	5714.142272	7.779648	-0.040403	4.092235
196.805196	5722.189085	7.784653	-0.040435	4.095009
196.938117	5730.187319	7.789658	-0.040465	4.097764
196.909214	5738.191814	7.794662	-0.040465	4.100517
197.152582	5746.210279	7.799667	-0.040516	4.103277
197.187578	5754.195871	7.804672	-0.040527	4.106021
197.356588	5762.249944	7.809677	-0.040564	4.108788
197.608231	5770.302752	7.814682	-0.040617	4.111555
197.629194	5778.330627	7.819686	-0.040626	4.114307
197.939679	5786.368526	7.824691	-0.040689	4.117065
197.962814	5794.322345	7.829696	-0.040699	4.119789
198.097918	5802.370384	7.834701	-0.040729	4.122544
198.410277	5810.333296	7.839706	-0.040793	4.125271
198.659716	5818.387096	7.844710	-0.040845	4.128026
198.790835	5826.436078	7.849715	-0.040874	4.130776
198.711832	5834.484398	7.854720	-0.040865	4.133522
199.024556	5842.496406	7.859725	-0.040929	4.136258
199.388292	5850.462534	7.864730	-0.041002	4.138977
199.234239	5858.515855	7.869734	-0.040979	4.141718
199.493636	5866.505605	7.874739	-0.041032	4.144440
199.772345	5874.523914	7.879744	-0.041089	4.147171
199.757870	5882.557028	7.884749	-0.041092	4.149901
199.896857	5890.622245	7.889754	-0.041123	4.152642
199.997987	5898.604927	7.894758	-0.041148	4.155353
200.238668	5906.627631	7.899763	-0.041198	4.158077
200.267822	5914.627973	7.904768	-0.041209	4.160790
200.541310	5922.615055	7.909773	-0.041265	4.163499
200.784466	5930.667530	7.914778	-0.041316	4.166228
200.919255	5938.659826	7.919782	-0.041346	4.168933
201.088776	5946.702393	7.924787	-0.041383	4.171654
201.493274	5954.691596	7.929792	-0.041464	4.174358
201.510535	5962.759144	7.934797	-0.041472	4.177083
201.549528	5970.733152	7.939802	-0.041485	4.179774
201.575992	5978.738664	7.944806	-0.041495	4.182474
201.915383	5986.815140	7.949811	-0.041564	4.185199
202.189189	5994.774895	7.954816	-0.041620	4.187883
202.270301	6002.818472	7.959821	-0.041641	4.190591
202.438785	6010.988914	7.964826	-0.041678	4.193341
202.506580	6018.930146	7.969830	-0.041696	4.196011
202.742298	6026.918567	7.974835	-0.041745	4.198697
202.905737	6034.906110	7.979840	-0.041781	4.201380
203.015295	6042.868868	7.984845	-0.041806	4.204052
203.118221	6050.952461	7.989850	-0.041831	4.206763
203.368296	6058.903476	7.994854	-0.041883	4.209430
203.636341	6066.989673	7.999859	-0.041938	4.212140
203.676472	6074.975217	8.004864	-0.041951	4.214812
203.889352	6082.998906	8.009869	-0.041996	4.217498
203.959612	6091.021820	8.014874	-0.042014	4.220179
204.152956	6098.998498	8.019878	-0.042056	4.222845
204.270161	6107.051811	8.024883	-0.042083	4.225534
204.319415	6115.028049	8.029888	-0.042098	4.228195
204.766210	6123.084804	8.034893	-0.042186	4.230885
204.829236	6131.130878	8.039898	-0.042203	4.233566
205.060556	6139.148130	8.044902	-0.042252	4.236237
205.241900	6147.132555	8.049907	-0.042291	4.238895
205.176319	6155.133825	8.054912	-0.042284	4.241555
205.125071	6163.119014	8.059917	-0.042280	4.244208
205.394033	6171.182924	8.064922	-0.042335	4.246888
205.454630	6179.226822	8.069926	-0.042352	4.249558
205.624531	6187.224748	8.074931	-0.042389	4.252212
205.992564	6195.239240	8.079936	-0.042463	4.254871
206.081189	6203.254303	8.084941	-0.042485	4.257527
206.102195	6211.307389	8.089946	-0.042494	4.260193
206.251337	6219.278053	8.094950	-0.042527	4.262831
206.547299	6227.292293	8.099955	-0.042588	4.265483
206.459629	6235.302014	8.104960	-0.042577	4.268129
206.747517	6243.362554	8.109965	-0.042636	4.270793
207.231107	6251.423119	8.114970	-0.042731	4.273457
207.333541	6259.482744	8.119974	-0.042756	4.276115
207.299956	6267.451450	8.124979	-0.042755	4.278741
207.390181	6275.443678	8.129984	-0.042777	4.281374
207.694646	6283.424032	8.134989	-0.042839	4.284004
207.937608	6291.498315	8.139994	-0.042890	4.286662
207.788782	6299.450742	8.144998	-0.042867	4.289275
208.207565	6307.508864	8.150003	-0.042951	4.291926
208.324998	6315.527270	8.155008	-0.042978	4.294560
208.421866	6323.574950	8.160013	-0.043001	4.297201
208.727223	6331.554951	8.165018	-0.043064	4.299820
208.779326	6339.555579	8.170022	-0.043079	4.302443
208.799141	6347.589541	8.175027	-0.043088	4.305074
208.975058	6355.635228	8.180032	-0.043126	4.307709
209.150317	6363.606700	8.185037	-0.043164	4.310318
209.194692	6371.696939	8.190042	-0.043178	4.312964
209.417450	6379.682906	8.195046	-0.043225	4.315575
209.662698	6387.673291	8.200051	-0.043276	4.318186
209.765068	6395.691006	8.205056	-0.043300	4.320803
209.888964	6403.681546	8.210061	-0.043328	4.323410
210.177347	6411.727906	8.215066	-0.043388	4.326034
210.088765	6419.751194	8.220070	-0.043376	4.328647
210.295602	6427.757467	8.225075	-0.043420	4.331255
210.264323	6435.778637	8.230080	-0.043420	4.333864
210.531088	6443.803972	8.235085	-0.043475	4.336476
210.473416	6451.813322	8.240090	-0.043470	4.339078
210.562916	6459.803191	8.245094	-0.043492	4.341673
210.976234	6467.820920	8.250099	-0.043574	4.344278
211.144105	6475.844887	8.255104	-0.043611	4.346882
211.216252	6483.882454	8.260109	-0.043629	4.349488
211.477806	6491.951864	8.265114	-0.043684	4.352104
211.414704	6500.015437	8.270118	-0.043677	4.354714
211.898574	6508.003399	8.275123	-0.043773	4.357302
211.753971	6515.946955	8.280128	-0.043751	4.359870
212.130319	6523.966094	8.285133	-0.043827	4.362464
212.341341	6531.921826	8.290138	-0.043871	4.365035
212.177941	6539.943718	8.295142	-0.043846	4.367623
212.470805	6548.027452	8.300147	-0.043906	4.370233
212.646730	6556.033109	8.305152	-0.043944	4.372815
212.874336	6564.026137	8.310157	-0.043992	4.375392
213.032003	6572.038843	8.315162	-0.044027	4.377973
213.233569	6580.039051	8.320166	-0.044070	4.380549
213.163459	6588.061586	8.325171	-0.044062	4.383129
213.063271	6596.069935	8.330176	-0.044049	4.385703
213.517707	6604.113981	8.335181	-0.044139	4.388290
213.694104	6612.209647	8.340186	-0.044177	4.390890
213.577572	6620.142020	8.345190	-0.044161	4.393435
213.935819	6628.205223	8.350195	-0.044233	4.396023
214.083177	6636.154121	8.355200	-0.044265	4.398571
214.073713	6644.230230	8.360205	-0.044269	4.401158
214.280255	6652.215833	8.365210	-0.044313	4.403716
214.256179	6660.177719	8.370214	-0.044314	4.406263
214.526986	6668.238099	8.375219	-0.044370	4.408842
214.834191	6676.281236	8.380224	-0.044432	4.411414
214.840248	6684.338823	8.385229	-0.044439	4.413987
215.116746	6692.412577	8.390234	-0.044496	4.416566
215.020401	6700.333400	8.395238	-0.044483	4.419092
215.396515	6708.404376	8.400243	-0.044559	4.421667
215.581849	6716.356634	8.405248	-0.044598	4.424202
215.649269	6724.412358	8.410253	-0.044616	4.426767
215.695965	6732.430899	8.415258	-0.044630	4.429320
216.031291	6740.441111	8.420262	-0.044698	4.431869
216.365463	6748.541560	8.425267	-0.044766	4.434446
216.436800	6756.533562	8.430272	-0.044785	4.436985
216.394665	6764.445193	8.435277	-0.044782	4.439497
216.481142	6772.513064	8.440282	-0.044804	4.442058
216.558244	6780.459724	8.445286	-0.044823	4.444578
216.846419	6788.557900	8.450291	-0.044882	4.447146
217.187101	6796.535003	8.455296	-0.044951	4.449675
217.331392	6804.589332	8.460301	-0.044983	4.452226
217.342819	6812.609557	8.465306	-0.044991	4.454764
217.674010	6820.603736	8.470310	-0.045058	4.457293
217.731921	6828.621743	8.475315	-0.045074	4.459827
217.836279	6836.632909	8.480320	-0.045099	4.462358
217.749565	6844.653900	8.485325	-0.045088	4.464890
218.165996	6852.650799	8.490330	-0.045171	4.467415
218.111166	6860.648874	8.495334	-0.045166	4.469937
218.353892	6868.723412	8.500339	-0.045217	4.472483
218.575940	6876.717619	8.505344	-0.045264	4.475002
218.623764	6884.698478	8.510349	-0.045278	4.477514
218.790832	6892.727239	8.515354	-0.045314	4.480041
219.092811	6900.721456	8.520358	-0.045376	4.482556
219.195831	6908.733265	8.525363	-0.045400	4.485074
219.152730	6916.793850	8.530368	-0.045398	4.487605
219.574009	6924.782761	8.535373	-0.045482	4.490115
219.769700	6932.822298	8.540378	-0.045523	4.492637
219.788408	6940.828281	8.545382	-0.045532	4.495148
219.944604	6948.864383	8.550387	-0.045567	4.497667
220.121551	6956.840060	8.555392	-0.045605	4.500165
220.329569	6964.845909	8.560397	-0.045649	4.502672
220.546735	6972.895159	8.565402	-0.045695	4.505191
220.637654	6980.921119	8.570407	-0.045717	4.507701
220.811717	6988.949905	8.575411	-0.045755	4.510210
220.882875	6996.993074	8.580416	-0.045774	4.512722
221.111996	7005.032506	8.585421	-0.045822	4.515232
221.651271	7013.014049	8.590426	-0.045928	4.517724
221.696329	7020.976904	8.595431	-0.045941	4.520207
221.674075	7028.986746	8.600435	-0.045943	4.522703
222.167706	7036.985289	8.605440	-0.046040	4.525195
222.095467	7045.002415	8.610445	-0.046032	4.527690
222.304791	7053.054159	8.615450	-0.046076	4.530196
222.516265	7061.053189	8.620455	-0.046121	4.532683
222.673931	7069.118347	8.625459	-0.046156	4.535190
222.717101	7077.111324	8.630464	-0.046169	4.537673
222.675912	7085.082047	8.635469	-0.046167	4.540147
223.056738	7093.139215	8.640474	-0.046243	4.542647
223.171169	7101.116866	8.645479	-0.046270	4.545121
223.290233	7109.170437	8.650483	-0.046297	4.547617
223.603745	7117.155889	8.655488	-0.046361	4.550091
223.687508	7125.227674	8.660493	-0.046382	4.552590
223.560268	7133.255493	8.665498	-0.046364	4.555073
223.831834	7141.241372	8.670503	-0.046420	4.557543
223.928516	7149.237523	8.675507	-0.046443	4.560015
223.972464	7157.255469	8.680512	-0.046457	4.562491
224.000346	7165.215146	8.685517	-0.046467	4.564949
224.174188	7173.269657	8.690522	-0.046505	4.567434
224.423399	7181.272660	8.695527	-0.046557	4.569902
224.499803	7189.336421	8.700531	-0.046576	4.572388
224.522049	7197.357136	8.705536	-0.046586	4.574859
224.636523	7205.374821	8.710541	-0.046613	4.577327
224.849821	7213.413856	8.715546	-0.046658	4.579801
224.948630	7221.408895	8.720551	-0.046682	4.582260
225.216910	7229.412934	8.725555	-0.046737	4.584720
225.373221	7237.446039	8.730560	-0.046771	4.587188
225.433957	7245.443056	8.735565	-0.046788	4.589644
225.653420	7253.502090	8.740570	-0.046834	4.592117
225.892882	7261.536002	8.745575	-0.046884	4.594581
225.977143	7269.585769	8.750579	-0.046905	4.597049
226.001103	7277.475878	8.755584	-0.046915	4.599466
226.205681	7285.513746	8.760589	-0.046959	4.601928
226.327149	7293.524451	8.765594	-0.046987	4.604379
226.334919	7301.564066	8.770599	-0.046993	4.606838
226.567590	7309.554751	8.775603	-0.047042	4.609281
226.660150	7317.606033	8.780608	-0.047065	4.611742
226.620314	7325.616685	8.785613	-0.047063	4.614188
226.991505	7333.657177	8.790618	-0.047137	4.616642
227.085981	7341.609906	8.795623	-0.047160	4.619068
227.557732	7349.684807	8.800627	-0.047253	4.621530
227.569028	7357.615326	8.805632	-0.047261	4.623947
227.819385	7365.687594	8.810637	-0.047313	4.626406
227.917874	7373.706659	8.815642	-0.047337	4.628847
227.970346	7381.721736	8.820647	-0.047352	4.631285
228.155021	7389.794653	8.825651	-0.047392	4.633740
228.363850	7397.808267	8.830656	-0.047436	4.636176
228.362855	7405.725059	8.835661	-0.047441	4.638580
228.661410	7413.814220	8.840666	-0.047502	4.641036
228.886453	7421.738854	8.845671	-0.047549	4.643441
229.099668	7429.771657	8.850675	-0.047594	4.645877
229.029180	7437.804946	8.855680	-0.047587	4.648312
229.130530	7445.844966	8.860685	-0.047611	4.650748
229.572728	7453.897479	8.865690	-0.047699	4.653186
229.333417	7461.863503	8.870695	-0.047659	4.655597
229.687729	7469.928477	8.875699	-0.047731	4.658036
229.936890	7477.915850	8.880704	-0.047783	4.660451
229.865849	7485.905237	8.885709	-0.047775	4.662865
230.063986	7493.919452	8.890714	-0.047817	4.665285
229.973238	7501.895338	8.895719	-0.047805	4.667693
230.202339	7509.955364	8.900723	-0.047854	4.670124
230.205991	7518.041452	8.905728	-0.047860	4.672563
230.567915	7526.042281	8.910733	-0.047932	4.674973
230.795491	7534.059169	8.915738	-0.047980	4.677388
230.999406	7541.949483	8.920743	-0.048023	4.679763
231.078909	7550.048710	8.925747	-0.048044	4.682200
231.220193	7557.973946	8.930752	-0.048075	4.684584
231.131263	7566.081691	8.935757	-0.048064	4.687021
231.260702	7574.045242	8.940762	-0.048094	4.689413
231.477841	7582.087286	8.945767	-0.048139	4.691828
231.667743	7590.104262	8.950771	-0.048180	4.694234
231.881683	7598.162022	8.955776	-0.048225	4.696650
231.904571	7606.066518	8.960781	-0.048235	4.699020
232.117825	7614.185784	8.965786	-0.048280	4.701453
232.072845	7622.154260	8.970791	-0.048277	4.703840
232.419130	7630.199501	8.975795	-0.048347	4.706247
232.771350	7638.143634	8.980800	-0.048418	4.708624
232.954983	7646.200280	8.985805	-0.048458	4.711033
233.008614	7654.295633	8.990810	-0.048473	4.713452
233.142737	7662.253659	8.995815	-0.048503	4.715829
233.443709	7670.273607	9.000819	-0.048565	4.718223
233.626991	7678.243397	9.005824	-0.048604	4.720601
233.734081	7686.237565	9.010829	-0.048629	4.722985
233.851789	7694.334376	9.015834	-0.048657	4.725399
233.855298	7702.319074	9.020839	-0.048663	4.727778
234.009296	7710.354273	9.025843	-0.048697	4.730171
234.456342	7718.414196	9.030848	-0.048786	4.732569
234.496179	7726.378969	9.035853	-0.048798	4.734939
234.743733	7734.413846	9.040858	-0.048850	4.737327
234.585672	7742.384744	9.045863	-0.048826	4.739697
234.941536	7750.440490	9.050867	-0.048897	4.742089
235.137137	7758.460927	9.055872	-0.048939	4.744470
235.088475	7766.493418	9.060877	-0.048936	4.746854
235.442756	7774.492160	9.065882	-0.049007	4.749225
235.489520	7782.506422	9.070887	-0.049021	4.751601
235.589042	7790.529525	9.075891	-0.049045	4.753978
235.561693	7798.580556	9.080896	-0.049045	4.756363
235.729332	7806.498627	9.085901	-0.049082	4.758706
235.899574	7814.608571	9.090906	-0.049119	4.761105
236.022451	7822.530983	9.095911	-0.049147	4.763447
236.318760	7830.580948	9.100915	-0.049208	4.765826
236.239534	7838.595551	9.105920	-0.049198	4.768194
236.379967	7846.561870	9.110925	-0.049230	4.770546
236.573134	7854.671460	9.115930	-0.049271	4.772938
236.565948	7862.620651	9.120935	-0.049275	4.775283
236.787118	7870.656178	9.125939	-0.049322	4.777652
236.915605	7878.637332	9.130944	-0.049351	4.780003
237.096623	7886.654988	9.135949	-0.049390	4.782364
237.147798	7894.673846	9.140954	-0.049405	4.784725
237.364630	7902.728705	9.145959	-0.049451	4.787094
237.692945	7910.736125	9.150963	-0.049517	4.789448
237.613639	7918.751366	9.155968	-0.049508	4.791804
237.677614	7926.803423	9.160973	-0.049525	4.794170
237.821051	7934.802169	9.165978	-0.049557	4.796518
237.872118	7942.747141	9.170983	-0.049572	4.798850
238.028062	7950.802959	9.175987	-0.049607	4.801212
238.117738	7958.809621	9.180992	-0.049629	4.803560
238.344774	7966.823426	9.185997	-0.049676	4.805908
238.449139	7974.847857	9.191002	-0.049701	4.808258
238.541424	7982.887803	9.196007	-0.049724	4.810612
238.844754	7990.271419	9.201011	-0.049785	4.812771
238.609578	7994.743270	9.206016	-0.049745	4.814080

238.695668	7997.247658	9.211021	-0.049762	4.814813
238.994184	7998.618905	9.216026	-0.049819	4.815212
239.038364	7999.017836	9.221031	-0.049828	4.815329
239.091779	7999.944333	9.226035	-0.049838	4.815599
239.089603	7999.949650	9.231040	-0.049838	4.815601
239.303125	7999.900815	9.236045	-0.049878	4.815586
239.360667	7999.940198	9.241050	-0.049889	4.815597
239.373000	7999.909450	9.246055	-0.049891	4.815588
239.445762	7999.949081	9.251059	-0.049905	4.815599
239.709028	7999.939489	9.256064	-0.049954	4.815595
239.730721	7999.906758	9.261069	-0.049958	4.815585
240.020049	7999.928552	9.266074	-0.050012	4.815590
239.854315	7999.919469	9.271079	-0.049982	4.815588
239.621364	7999.923174	9.276083	-0.049938	4.815591
239.796114	7999.963393	9.281088	-0.049971	4.815601
239.970841	7999.927808	9.286093	-0.050004	4.815590
239.898698	7999.953342	9.291098	-0.049991	4.815598
239.814795	7999.910355	9.296103	-0.049975	4.815586
239.986432	7999.919561	9.301107	-0.050007	4.815588
239.961300	7999.949061	9.306112	-0.050003	4.815596
239.966455	7999.918197	9.311117	-0.050004	4.815587
239.979410	7999.964330	9.316122	-0.050006	4.815601
239.966340	7999.931034	9.321127	-0.050004	4.815591
240.000125	7999.946544	9.326131	-0.050011	4.815596
240.135640	7999.961570	9.331136	-0.050036	4.815599
240.188848	7999.929351	9.336141	-0.050046	4.815590
240.202960	7999.974435	9.341146	-0.050049	4.815603
240.185791	7999.921855	9.346151	-0.050046	4.815587
240.288178	7999.925667	9.351155	-0.050065	4.815588
240.395135	7999.918876	9.356160	-0.050085	4.815586
240.422491	7999.952432	9.361165	-0.050090	4.815595
240.531266	7999.964889	9.366170	-0.050111	4.815598
240.582981	7999.940119	9.371175	-0.050121	4.815591
240.453982	7999.959391	9.376179	-0.050097	4.815597
240.481832	7999.941706	9.381184	-0.050102	4.815592
240.499753	7999.953756	9.386189	-0.050106	4.815595
240.426404	7999.964322	9.391194	-0.050092	4.815599
240.480787	7999.940663	9.396199	-0.050102	4.815592
240.647124	7999.951920	9.401203	-0.050133	4.815594
240.502434	7999.933568	9.406208	-0.050107	4.815589
240.277297	7999.935264	9.411213	-0.050065	4.815591
240.425876	7999.952638	9.416218	-0.050093	4.815595
240.449849	7999.927417	9.421223	-0.050097	4.815588
240.523453	7999.943574	9.426227	-0.050111	4.815592
240.588352	7999.946777	9.431232	-0.050123	4.815593
240.711079	7999.955191	9.436237	-0.050146	4.815595
240.727896	7999.998185	9.441242	-0.050150	4.815607
240.529835	8000.003523	9.446247	-0.050113	4.815610
240.659976	7999.974688	9.451251	-0.050137	4.815601
240.821463	7999.957039	9.456256	-0.050168	4.815595
240.678165	8000.019853	9.461261	-0.050141	4.815614
240.773449	8000.024618	9.466266	-0.050159	4.815615
240.942376	8000.014564	9.471271	-0.050191	4.815611
240.916724	7999.983198	9.476275	-0.050186	4.815602
240.803227	8000.027279	9.481280	-0.050165	4.815615
240.791073	7999.971575	9.486285	-0.050163	4.815599
241.024980	7999.989269	9.491290	-0.050207	4.815603
240.863838	7999.933280	9.496295	-0.050177	4.815587
240.913696	7999.944781	9.501299	-0.050186	4.815591
241.086377	7999.917705	9.506304	-0.050219	4.815582
241.011497	7999.931450	9.511309	-0.050205	4.815586
240.977915	7999.950136	9.516314	-0.050199	4.815592
240.994032	7999.916246	9.521319	-0.050202	4.815582
241.153723	7999.947682	9.526323	-0.050232	4.815590
241.023471	7999.958392	9.531328	-0.050208	4.815594
241.080361	7999.929434	9.536333	-0.050218	4.815585
241.029883	7999.955320	9.541338	-0.050209	4.815593
240.868493	7999.932426	9.546343	-0.050179	4.815587
240.881261	7999.957204	9.551347	-0.050182	4.815594
241.024728	7999.923247	9.556352	-0.050209	4.815584
240.872830	7999.905846	9.561357	-0.050180	4.815579
240.912124	7999.956679	9.566362	-0.050188	4.815594
240.984725	7999.967481	9.571367	-0.050202	4.815597
241.111603	7999.965286	9.576371	-0.050225	4.815596
240.990471	7999.975076	9.581376	-0.050203	4.815599
240.978202	7999.930048	9.586381	-0.050201	4.815586
241.176649	7999.973858	9.591386	-0.050238	4.815598
240.876450	7999.931625	9.596391	-0.050182	4.815587
241.096543	7999.958704	9.601395	-0.050223	4.815594
241.080599	7999.945646	9.606400	-0.050221	4.815590
241.071964	7999.940181	9.611405	-0.050219	4.815588
241.212075	7999.952081	9.616410	-0.050245	4.815591
241.240205	7999.929062	9.621415	-0.050251	4.815584
241.442230	7999.946238	9.626419	-0.050289	4.815588
241.165874	7999.933220	9.631424	-0.050237	4.815586
241.266977	7999.922065	9.636429	-0.050256	4.815582
241.402619	7999.960584	9.641434	-0.050282	4.815593
241.163601	7999.916142	9.646439	-0.050237	4.815581
241.252355	7999.952831	9.651443	-0.050254	4.815591
241.329847	7999.921006	9.656448	-0.050269	4.815582
241.305681	7999.929168	9.661453	-0.050264	4.815584
241.390483	7999.987148	9.666458	-0.050280	4.815601
241.349614	7999.984362	9.671463	-0.050273	4.815600
241.473606	7999.990662	9.676467	-0.050296	4.815601
241.157862	7999.936431	9.681472	-0.050237	4.815587
241.127689	7999.931684	9.686477	-0.050232	4.815586
241.441825	7999.991254	9.691482	-0.050291	4.815601
241.260721	7999.927467	9.696487	-0.050257	4.815584
241.231009	7999.955825	9.701491	-0.050252	4.815592
241.199047	8000.005501	9.706496	-0.050246	4.815607
241.325939	7999.976614	9.711501	-0.050270	4.815598
241.345481	7999.967336	9.716506	-0.050273	4.815595
241.389785	7999.911482	9.721511	-0.050282	4.815578
241.509840	7999.919852	9.726515	-0.050304	4.815580
241.524352	7999.917966	9.731520	-0.050307	4.815580
241.299510	7999.925004	9.736525	-0.050265	4.815583
241.539517	7999.981235	9.741530	-0.050310	4.815598
241.492152	7999.933500	9.746535	-0.050302	4.815584
241.388104	7999.964922	9.751539	-0.050282	4.815594
241.442543	7999.955143	9.756544	-0.050293	4.815591
241.584135	7999.925427	9.761549	-0.050319	4.815582
241.530341	7999.963004	9.766554	-0.050309	4.815593
241.468013	7999.923567	9.771559	-0.050298	4.815582
241.574289	7999.939188	9.776563	-0.050318	4.815586
241.502429	7999.935899	9.781568	-0.050305	4.815585
241.524149	7999.940536	9.786573	-0.050309	4.815586
241.717151	7999.953296	9.791578	-0.050345	4.815589
241.376598	7999.928557	9.796583	-0.050282	4.815583
241.463431	7999.929982	9.801587	-0.050298	4.815583
241.603209	7999.917319	9.806592	-0.050324	4.815579
241.495239	7999.909172	9.811597	-0.050304	4.815577
241.386640	7999.983228	9.816602	-0.050284	4.815599
241.458860	7999.938504	9.821607	-0.050298	4.815586
241.723817	7999.932146	9.826611	-0.050347	4.815583
241.749005	7999.918689	9.831616	-0.050352	4.815579
241.571966	7999.958534	9.836621	-0.050319	4.815591
241.668009	7999.948364	9.841626	-0.050337	4.815588
241.646118	7999.920262	9.846631	-0.050333	4.815580
241.589334	7999.966332	9.851635	-0.050323	4.815593
241.685785	7999.959371	9.856640	-0.050341	4.815591
241.753072	7999.924176	9.861645	-0.050354	4.815580
241.719857	7999.950343	9.866650	-0.050348	4.815588
241.755842	7999.913572	9.871655	-0.050355	4.815577
241.799653	7999.953803	9.876659	-0.050363	4.815589
241.809251	7999.941160	9.881664	-0.050365	4.815585
241.602384	7999.925000	9.886669	-0.050327	4.815581
241.804334	7999.971004	9.891674	-0.050364	4.815594
241.735873	7999.917587	9.896679	-0.050352	4.815578
241.658157	7999.918473	9.901683	-0.050337	4.815579
241.844714	7999.908706	9.906688	-0.050372	4.815575
242.026118	7999.919142	9.911693	-0.050406	4.815577
241.944057	7999.941312	9.916698	-0.050391	4.815584
241.623979	7999.890213	9.921703	-0.050332	4.815571
242.066307	7999.941191	9.926707	-0.050414	4.815584
242.114852	7999.931317	9.931712	-0.050423	4.815581
241.814448	7999.925380	9.936717	-0.050368	4.815580
242.073114	7999.957359	9.941722	-0.050416	4.815588
242.148428	7999.919091	9.946727	-0.050430	4.815577
242.021470	7999.961885	9.951731	-0.050407	4.815590
241.979943	7999.945208	9.956736	-0.050399	4.815585
242.061720	7999.954025	9.961741	-0.050415	4.815587
242.014048	7999.963942	9.966746	-0.050406	4.815591
241.691163	7999.928812	9.971751	-0.050346	4.815582
241.925676	7999.960397	9.976755	-0.050390	4.815590
241.918328	7999.953885	9.981760	-0.050388	4.815588
241.916507	7999.910093	9.986765	-0.050388	4.815575
242.001193	7999.933905	9.991770	-0.050404	4.815582
242.001925	7999.901900	9.996775	-0.050404	4.815572
242.059062	7999.929535	10.001779	-0.050415	4.815580
241.956134	7999.918266	10.006784	-0.050396	4.815577
241.977557	7999.917561	10.011789	-0.050400	4.815577
242.236632	7999.945275	10.016794	-0.050449	4.815584
241.900165	7999.935549	10.021799	-0.050386	4.815583
241.988822	7999.962629	10.026803	-0.050403	4.815590
242.096762	7999.914215	10.031808	-0.050423	4.815576
242.101147	7999.908961	10.036813	-0.050424	4.815574
241.984352	7999.951921	10.041818	-0.050403	4.815587
242.035502	7999.916463	10.046823	-0.050412	4.815577
241.982718	7999.964734	10.051827	-0.050403	4.815591
241.912775	7999.967882	10.056832	-0.050390	4.815592
241.978351	7999.949743	10.061837	-0.050402	4.815587
242.116392	7999.961610	10.066842	-0.050428	4.815589
241.854340	7999.918926	10.071847	-0.050379	4.815578
242.003709	7999.957670	10.076851	-0.050407	4.815589
242.214671	7999.944029	10.081856	-0.050447	4.815584
242.107831	7999.927359	10.086861	-0.050427	4.815579
242.064773	7999.973652	10.091866	-0.050419	4.815593
242.277946	7999.912000	10.096871	-0.050459	4.815574
241.886954	7999.964383	10.101875	-0.050386	4.815591
241.867424	7999.980095	10.106880	-0.050383	4.815596
241.890405	7999.946316	10.111885	-0.050387	4.815586
241.983425	7999.969195	10.116890	-0.050405	4.815592
241.956916	7999.943153	10.121895	-0.050400	4.815585
242.093224	7999.971008	10.126899	-0.050426	4.815592
242.255422	7999.974726	10.131904	-0.050456	4.815592
242.153219	7999.928234	10.136909	-0.050437	4.815579
242.143080	7999.940896	10.141914	-0.050435	4.815583
242.282917	7999.933573	10.146919	-0.050462	4.815580
242.176916	7999.954286	10.151923	-0.050442	4.815587
242.164811	7999.944493	10.156928	-0.050440	4.815584
242.257127	7999.913976	10.161933	-0.050457	4.815575
242.281994	7999.917597	10.166938	-0.050462	4.815576
242.394328	7999.931182	10.171943	-0.050483	4.815579
242.247217	7999.945888	10.176947	-0.050456	4.815584
242.372530	7999.956480	10.181952	-0.050479	4.815587
242.020345	7999.931551	10.186957	-0.050414	4.815581
242.091697	8000.007464	10.191962	-0.050427	4.815603
242.311079	7999.930965	10.196967	-0.050468	4.815579
242.297350	7999.943568	10.201971	-0.050466	4.815583
242.129464	7999.935515	10.206976	-0.050435	4.815582
242.076747	7999.942146	10.211981	-0.050425	4.815584
242.257515	7999.962181	10.216986	-0.050459	4.815589
242.065671	7999.965483	10.221991	-0.050423	4.815591
242.102584	7999.992790	10.226995	-0.050431	4.815598
242.174273	8000.009985	10.232000	-0.050444	4.815603
242.176344	7999.947037	10.237005	-0.050445	4.815585
242.231637	7999.962897	10.242010	-0.050455	4.815589
242.177116	7999.946009	10.247015	-0.050445	4.815584
242.185374	7999.949360	10.252019	-0.050447	4.815585
242.216876	7999.928531	10.257024	-0.050453	4.815579
242.195423	7999.917519	10.262029	-0.050449	4.815576
242.445669	7999.952565	10.267034	-0.050496	4.815585
242.306671	7999.977012	10.272039	-0.050470	4.815593
242.163698	7999.984311	10.277043	-0.050443	4.815596
242.420482	7999.970348	10.282048	-0.050491	4.815590
242.490763	7999.948014	10.287053	-0.050505	4.815583
242.255417	8000.029620	10.292058	-0.050461	4.815608
242.238380	7999.984513	10.297063	-0.050458	4.815595
242.510664	7999.980411	10.302067	-0.050509	4.815593
242.476891	7999.948912	10.307072	-0.050503	4.815584
242.271903	7999.942390	10.312077	-0.050465	4.815583
242.520551	7999.992358	10.317082	-0.050511	4.815596
242.571843	7999.938752	10.322087	-0.050521	4.815580
242.295420	7999.959897	10.327091	-0.050470	4.815588
242.445852	8000.009337	10.332096	-0.050498	4.815601
242.313410	7999.927118	10.337101	-0.050473	4.815578
242.410947	7999.999187	10.342106	-0.050492	4.815599
242.427581	7999.952491	10.347111	-0.050495	4.815585
242.452159	7999.963582	10.352115	-0.050500	4.815588
242.356004	7999.970574	10.357120	-0.050482	4.815591
242.200854	7999.969134	10.362125	-0.050453	4.815591
242.534600	7999.994860	10.367130	-0.050515	4.815597
242.449777	7999.975343	10.372135	-0.050500	4.815592
242.586879	7999.948757	10.377139	-0.050525	4.815583
242.512007	7999.982789	10.382144	-0.050512	4.815593
242.415324	7999.960944	10.387149	-0.050494	4.815587
242.533579	7999.982099	10.392154	-0.050516	4.815593
242.497523	7999.951631	10.397159	-0.050509	4.815584
242.597077	7999.963940	10.402163	-0.050528	4.815587
242.849984	7999.994760	10.407168	-0.050575	4.815595
242.383326	7999.958357	10.412173	-0.050489	4.815587
242.680663	7999.989898	10.417178	-0.050544	4.815595
242.619271	8000.012404	10.422183	-0.050533	4.815601
242.512203	8000.001068	10.427187	-0.050513	4.815599
242.364665	8000.100117	10.432192	-0.050486	4.815628
242.604709	7999.951348	10.437197	-0.050531	4.815584
242.567867	8000.010556	10.442202	-0.050524	4.815601
242.285576	7999.956865	10.447207	-0.050472	4.815587
242.421184	7999.967625	10.452211	-0.050497	4.815589
242.559914	7999.969894	10.457216	-0.050523	4.815589
242.234016	7999.919765	10.462221	-0.050462	4.815576
242.572743	7999.974401	10.467226	-0.050526	4.815591
242.697985	7999.945487	10.472231	-0.050549	4.815582
242.664310	7999.968443	10.477235	-0.050543	4.815588
242.397512	7999.971593	10.482240	-0.050493	4.815591
242.457135	7999.948019	10.487245	-0.050505	4.815583
242.649702	7999.972518	10.492250	-0.050541	4.815590
242.491551	7999.960351	10.497255	-0.050511	4.815587
242.767858	7999.966992	10.502259	-0.050563	4.815587
242.795053	7999.949297	10.507264	-0.050568	4.815582
242.458070	7999.937426	10.512269	-0.050506	4.815580
242.611975	7999.990125	10.517274	-0.050535	4.815595
242.652141	7999.986521	10.522279	-0.050542	4.815594
242.807723	7999.957032	10.527283	-0.050571	4.815584
242.781524	7999.961959	10.532288	-0.050567	4.815586
242.790707	7999.925819	10.537293	-0.050568	4.815575
242.863559	7999.977201	10.542298	-0.050582	4.815590
242.642497	7999.929843	10.547303	-0.050541	4.815577
242.784928	7999.967408	10.552307	-0.050568	4.815587
242.832219	7999.956445	10.557312	-0.050577	4.815584
242.753814	7999.944507	10.562317	-0.050562	4.815581
242.797056	7999.975120	10.567322	-0.050571	4.815590
242.662257	7999.952655	10.572327	-0.050546	4.815584
242.716981	7999.966372	10.577331	-0.050556	4.815587
242.546580	7999.965751	10.582336	-0.050524	4.815588
242.481573	7999.958301	10.587341	-0.050512	4.815586
242.733308	7999.994440	10.592346	-0.050559	4.815596
242.553091	7999.946679	10.597351	-0.050526	4.815582
242.675332	7999.944409	10.602355	-0.050549	4.815581
242.612125	8000.006391	10.607360	-0.050537	4.815600
242.640730	7999.989786	10.612365	-0.050543	4.815595
242.704863	7999.987640	10.617370	-0.050555	4.815594
242.679428	7999.984037	10.622375	-0.050550	4.815593
242.579624	7999.970683	10.627379	-0.050532	4.815589
242.569372	7999.992952	10.632384	-0.050530	4.815596
242.702390	7999.950284	10.637389	-0.050555	4.815583
242.733436	7999.977496	10.642394	-0.050561	4.815591
242.596376	7999.964604	10.647399	-0.050536	4.815587
242.603265	8000.007439	10.652403	-0.050537	4.815600
242.749636	8000.011968	10.657408	-0.050565	4.815601
242.718097	7999.948473	10.662413	-0.050559	4.815582
242.599009	8000.003140	10.667418	-0.050537	4.815599
242.819809	7999.970441	10.672423	-0.050578	4.815588
242.956028	7999.979076	10.677427	-0.050604	4.815590
242.852163	7999.988078	10.682432	-0.050584	4.815593
242.783017	7999.958139	10.687437	-0.050572	4.815585
242.957603	8000.007972	10.692442	-0.050604	4.815598
242.849404	7999.960314	10.697447	-0.050584	4.815585
242.785640	7999.957155	10.702451	-0.050573	4.815584
242.744966	7999.943695	10.707456	-0.050565	4.815581
242.606147	7999.946790	10.712461	-0.050540	4.815582
242.773293	7999.966605	10.717466	-0.050571	4.815587
242.717514	7999.927274	10.722471	-0.050561	4.815576
242.769525	7999.960165	10.727475	-0.050570	4.815585
242.768120	7999.969766	10.732480	-0.050570	4.815588
242.588618	7999.949777	10.737485	-0.050537	4.815583
242.813692	7999.968399	10.742490	-0.050579	4.815587
242.793886	7999.951007	10.747495	-0.050576	4.815582
242.977558	7999.979633	10.752499	-0.050610	4.815590
242.932146	7999.965028	10.757504	-0.050602	4.815586
242.869164	7999.933053	10.762509	-0.050590	4.815577
242.952049	7999.984598	10.767514	-0.050606	4.815592
243.042823	7999.945514	10.772519	-0.050623	4.815580
243.151359	7999.959038	10.777523	-0.050643	4.815583
243.044943	7999.993624	10.782528	-0.050623	4.815594
242.897037	7999.950659	10.787533	-0.050596	4.815582
243.070175	7999.972707	10.792538	-0.050628	4.815587
242.868573	7999.926733	10.797543	-0.050591	4.815575
242.966039	7999.959296	10.802547	-0.050609	4.815584
243.065941	7999.969477	10.807552	-0.050628	4.815587
242.898950	7999.922998	10.812557	-0.050597	4.815574
242.924524	7999.964001	10.817562	-0.050602	4.815586
242.916839	7999.963890	10.822567	-0.050601	4.815586
242.975201	7999.963785	10.827571	-0.050612	4.815585
242.992414	7999.953401	10.832576	-0.050615	4.815582
242.933182	7999.950317	10.837581	-0.050604	4.815582
242.988025	7999.959764	10.842586	-0.050615	4.815584
243.042352	7999.959594	10.847591	-0.050625	4.815584
243.125680	7999.997266	10.852595	-0.050641	4.815594
243.170995	8000.026846	10.857600	-0.050649	4.815603
243.090210	7999.961481	10.862605	-0.050634	4.815584
243.112584	7999.973604	10.867610	-0.050639	4.815587
242.953291	7999.965688	10.872615	-0.050609	4.815586
243.031861	7999.947760	10.877619	-0.050624	4.815580
243.122355	7999.973804	10.882624	-0.050641	4.815587
242.829828	7999.947706	10.887629	-0.050587	4.815581
242.947679	7999.972059	10.892634	-0.050609	4.815588
243.040014	8000.003471	10.897639	-0.050626	4.815596
242.879684	7999.992335	10.902643	-0.050597	4.815594
243.141737	7999.992340	10.907648	-0.050645	4.815593
243.137708	7999.958120	10.912653	-0.050645	4.815583
243.015918	7999.976441	10.917658	-0.050622	4.815589
242.991707	7999.960044	10.922663	-0.050618	4.815584
243.034242	7999.968224	10.927667	-0.050626	4.815586
242.893054	7999.981958	10.932672	-0.050600	4.815591
242.960012	7999.980925	10.937677	-0.050613	4.815590
243.255253	7999.990011	10.942682	-0.050668	4.815592
243.199957	7999.984855	10.947687	-0.050658	4.815590
242.890335	7999.977698	10.952691	-0.050600	4.815590
242.997501	7999.993335	10.957696	-0.050620	4.815594
243.039538	7999.964136	10.962701	-0.050628	4.815585
243.045075	7999.988798	10.967706	-0.050629	4.815592
243.102471	7999.935290	10.972711	-0.050640	4.815576
243.319533	7999.945240	10.977715	-0.050681	4.815578
243.092206	7999.943692	10.982720	-0.050639	4.815579
242.909890	7999.956758	10.987725	-0.050605	4.815583
242.961264	7999.999249	10.992730	-0.050615	4.815596
243.319116	7999.994405	10.997735	-0.050681	4.815592
243.179608	7999.992150	11.002739	-0.050656	4.815592
243.285727	8000.022719	11.007744	-0.050675	4.815601
243.159258	7999.970491	11.012749	-0.050652	4.815586
243.123124	7999.977392	11.017754	-0.050645	4.815588
243.032956	7999.972736	11.022759	-0.050629	4.815587
243.159306	7999.971601	11.027763	-0.050653	4.815587
243.326048	8000.009563	11.032768	-0.050684	4.815597
243.105880	7999.991047	11.037773	-0.050643	4.815592
243.045888	8000.002898	11.042778	-0.050632	4.815596
243.085144	7999.967247	11.047783	-0.050639	4.815586
242.988409	7999.975297	11.052787	-0.050621	4.815588
243.054891	7999.975325	11.057792	-0.050634	4.815588
243.146092	7999.949060	11.062797	-0.050651	4.815580
243.164683	7999.979273	11.067802	-0.050655	4.815589
243.243826	8000.014742	11.072807	-0.050670	4.815599
243.173557	7999.991190	11.077811	-0.050657	4.815592
243.107046	8000.001868	11.082816	-0.050645	4.815596
243.049149	7999.976382	11.087821	-0.050634	4.815588
243.277416	7999.988650	11.092826	-0.050677	4.815591
243.380832	7999.967923	11.097831	-0.050696	4.815584
242.960020	7999.977109	11.102835	-0.050618	4.815589
243.093225	7999.993170	11.107840	-0.050643	4.815593
243.170310	7999.943185	11.112845	-0.050657	4.815578
243.300993	8000.013661	11.117850	-0.050682	4.815598
243.192728	7999.977745	11.122855	-0.050662	4.815588
243.200825	7999.959739	11.127859	-0.050663	4.815583
243.285802	8000.034810	11.132864	-0.050679	4.815604
243.124076	7999.965993	11.137869	-0.050649	4.815585
243.292730	7999.981562	11.142874	-0.050681	4.815589
243.337653	8000.003662	11.147879	-0.050690	4.815595
243.228912	7999.968807	11.152883	-0.050669	4.815585
243.079367	7999.974930	11.157888	-0.050642	4.815588
243.011456	7999.958891	11.162893	-0.050629	4.815583
243.145635	8000.003797	11.167898	-0.050654	4.815596
243.208382	7999.985612	11.172903	-0.050666	4.815590
243.206267	7999.988795	11.177907	-0.050666	4.815591
243.367050	7999.999965	11.182912	-0.050696	4.815594
243.369698	7999.974396	11.187917	-0.050697	4.815586
243.393255	8000.007894	11.192922	-0.050701	4.815596
243.450640	8000.017383	11.197927	-0.050712	4.815598
243.248799	7999.987420	11.202931	-0.050675	4.815591
243.316150	8000.031239	11.207936	-0.050687	4.815603
243.266954	7999.989878	11.212941	-0.050678	4.815591
243.379094	7999.999190	11.217946	-0.050699	4.815593
243.051894	7999.976798	11.222951	-0.050639	4.815588
243.393024	7999.966344	11.227955	-0.050702	4.815584
243.370684	7999.961723	11.232960	-0.050698	4.815582
243.291819	7999.954048	11.237965	-0.050684	4.815581
243.277963	8000.025376	11.242970	-0.050681	4.815601
243.483382	8000.000969	11.247975	-0.050720	4.815593
243.510686	7999.997156	11.252979	-0.050725	4.815592
243.370071	7999.982069	11.257984	-0.050699	4.815588
243.340395	7999.939958	11.262989	-0.050694	4.815576
243.515119	7999.957762	11.267994	-0.050726	4.815581
243.388363	7999.980273	11.272999	-0.050703	4.815588
243.328415	7999.941940	11.278003	-0.050692	4.815577
243.413909	7999.974309	11.283008	-0.050708	4.815586
243.195684	7999.954758	11.288013	-0.050667	4.815581
243.244039	8000.006810	11.293018	-0.050677	4.815596
243.221190	7999.968013	11.298023	-0.050673	4.815585
243.298663	7999.971422	11.303027	-0.050687	4.815586
243.092459	7999.990505	11.308032	-0.050649	4.815592
243.049925	7999.947117	11.313037	-0.050641	4.815580
243.353777	7999.988376	11.318042	-0.050698	4.815590
243.374599	8000.002610	11.323047	-0.050702	4.815594
243.372382	7999.997249	11.328051	-0.050702	4.815593
243.340046	7999.989262	11.333056	-0.050696	4.815591
243.409541	7999.959441	11.338061	-0.050709	4.815582
243.460406	7999.975231	11.343066	-0.050719	4.815586
243.535522	7999.926282	11.348071	-0.050733	4.815571
243.502614	7999.962064	11.353075	-0.050727	4.815582
243.596756	7999.971084	11.358080	-0.050744	4.815584
243.521031	7999.957053	11.363085	-0.050730	4.815580
243.521636	7999.968822	11.368090	-0.050731	4.815584
243.382753	7999.960170	11.373095	-0.050705	4.815582
243.295344	7999.968372	11.378099	-0.050689	4.815585
243.344309	7999.995876	11.383104	-0.050698	4.815592
243.487985	7999.961923	11.388109	-0.050725	4.815582
243.464205	8000.017073	11.393114	-0.050721	4.815598
243.350887	7999.965059	11.398119	-0.050700	4.815583
243.422002	7999.958755	11.403123	-0.050713	4.815581
243.413307	7999.970373	11.408128	-0.050712	4.815585
243.255926	7999.940066	11.413133	-0.050683	4.815577
243.400693	7999.976602	11.418138	-0.050710	4.815587
243.636515	8000.000739	11.423143	-0.050754	4.815592
243.378819	7999.970935	11.428147	-0.050706	4.815585
243.622209	7999.981314	11.433152	-0.050751	4.815587
243.560832	7999.969652	11.438157	-0.050740	4.815584
243.408619	7999.982139	11.443162	-0.050712	4.815588
243.538745	7999.994947	11.448167	-0.050736	4.815591
243.338128	7999.982087	11.453171	-0.050699	4.815588
243.428633	7999.989980	11.458176	-0.050716	4.815590
243.210812	7999.937334	11.463181	-0.050676	4.815576
243.403260	7999.973578	11.468186	-0.050712	4.815586
243.466232	7999.958600	11.473191	-0.050724	4.815581
243.448780	7999.979685	11.478195	-0.050721	4.815587
243.420198	7999.954675	11.483200	-0.050715	4.815580
243.527846	7999.952169	11.488205	-0.050736	4.815579
243.555198	7999.979322	11.493210	-0.050741	4.815587
243.578549	7999.959428	11.498215	-0.050745	4.815581
243.665660	7999.971536	11.503219	-0.050762	4.815584
243.693745	7999.976278	11.508224	-0.050767	4.815585
243.368570	7999.981680	11.513229	-0.050707	4.815588
243.472031	7999.992987	11.518234	-0.050726	4.815591
243.498481	7999.941110	11.523239	-0.050731	4.815576
243.316628	7999.948844	11.528243	-0.050698	4.815579
243.421923	7999.960180	11.533248	-0.050717	4.815582
243.484438	7999.948398	11.538253	-0.050729	4.815578
243.425839	7999.981627	11.543258	-0.050718	4.815588
243.350072	7999.971866	11.548263	-0.050704	4.815585
243.514755	7999.939322	11.553267	-0.050735	4.815575
243.500761	7999.975412	11.558272	-0.050733	4.815586
243.430788	7999.964678	11.563277	-0.050720	4.815583
243.466564	7999.995171	11.568282	-0.050727	4.815592
243.555781	7999.959264	11.573287	-0.050744	4.815581
243.602893	7999.962180	11.578291	-0.050752	4.815581
243.669858	7999.981435	11.583296	-0.050765	4.815587
243.719046	7999.952352	11.588301	-0.050774	4.815578
243.676808	7999.989050	11.593306	-0.050767	4.815589
243.428880	7999.982895	11.598311	-0.050721	4.815588
243.621448	7999.955076	11.603315	-0.050757	4.815579
243.734527	8000.002844	11.608320	-0.050778	4.815592
243.392106	7999.950306	11.613325	-0.050714	4.815579
243.425970	7999.965819	11.618330	-0.050721	4.815583
243.752808	8000.041622	11.623335	-0.050782	4.815604
243.485703	7999.990309	11.628339	-0.050732	4.815590
243.559334	7999.991520	11.633344	-0.050746	4.815590
243.668618	7999.963415	11.638349	-0.050767	4.815581
243.635002	7999.991711	11.643354	-0.050760	4.815590
243.502381	7999.983161	11.648359	-0.050736	4.815588
243.558759	7999.958466	11.653363	-0.050747	4.815580
243.591451	7999.964350	11.658368	-0.050753	4.815582
243.515610	7999.938572	11.663373	-0.050739	4.815575
243.534751	7999.961320	11.668378	-0.050743	4.815581
243.641726	7999.956667	11.673383	-0.050763	4.815579
243.496160	7999.963923	11.678387	-0.050736	4.815582
243.443084	7999.990835	11.683392	-0.050726	4.815590
243.510004	7999.955633	11.688397	-0.050739	4.815580
243.653378	7999.970793	11.693402	-0.050765	4.815583
243.619736	7999.984140	11.698407	-0.050759	4.815587
243.719769	7999.979374	11.703411	-0.050778	4.815586
243.630915	7999.973672	11.708416	-0.050762	4.815584
243.467831	7999.948610	11.713421	-0.050732	4.815578
243.544044	8000.020336	11.718426	-0.050746	4.815598
243.449610	8000.007068	11.723431	-0.050729	4.815595
243.551260	7999.967092	11.728435	-0.050748	4.815583
243.472982	7999.978646	11.733440	-0.050733	4.815587
243.467071	7999.965751	11.738445	-0.050732	4.815583
243.515942	7999.997524	11.743450	-0.050741	4.815592
243.451414	7999.958049	11.748455	-0.050730	4.815581
243.590214	7999.962456	11.753459	-0.050756	4.815581
243.690663	8000.011086	11.758464	-0.050774	4.815595
243.464399	7999.997809	11.763469	-0.050733	4.815592
243.420458	8000.004582	11.768474	-0.050724	4.815594
243.622749	8000.028174	11.773479	-0.050762	4.815600
243.690474	7999.965224	11.778483	-0.050775	4.815582
243.532053	8000.007507	11.783488	-0.050746	4.815595
243.564632	7999.993102	11.788493	-0.050752	4.815590
243.604985	8000.003382	11.793498	-0.050760	4.815593
243.491290	7999.991936	11.798503	-0.050739	4.815590
243.424793	7999.968445	11.803507	-0.050726	4.815584
243.541611	8000.025883	11.808512	-0.050748	4.815600
243.514043	7999.965654	11.813517	-0.050743	4.815582
243.600345	7999.961732	11.818522	-0.050760	4.815581
243.667089	7999.969238	11.823527	-0.050772	4.815583
243.733785	7999.960727	11.828531	-0.050785	4.815580
243.772562	7999.994473	11.833536	-0.050792	4.815590
243.660580	7999.964903	11.838541	-0.050771	4.815582
243.730903	7999.990619	11.843546	-0.050785	4.815589
243.767206	7999.975207	11.848551	-0.050792	4.815584
243.636984	7999.947476	11.853555	-0.050767	4.815577
243.904411	8000.006297	11.858560	-0.050817	4.815592
243.593681	7999.986307	11.863565	-0.050760	4.815588
243.796155	8000.017376	11.868570	-0.050798	4.815596
243.836463	8000.010571	11.873575	-0.050805	4.815594
243.721652	7999.980955	11.878579	-0.050784	4.815586
243.754483	8000.007130	11.883584	-0.050790	4.815593
243.693974	7999.964516	11.888589	-0.050779	4.815581
243.598860	7999.996083	11.893594	-0.050762	4.815591
243.581516	7999.948833	11.898599	-0.050759	4.815577
243.629177	7999.959232	11.903603	-0.050768	4.815580
243.745820	8000.014532	11.908608	-0.050790	4.815596
243.766405	7999.968967	11.913613	-0.050793	4.815582
243.693595	7999.997693	11.918618	-0.050780	4.815591
243.920971	8000.069744	11.923623	-0.050823	4.815611
243.729493	7999.998305	11.928627	-0.050787	4.815591
243.707587	8000.026792	11.933632	-0.050783	4.815599
243.724090	8000.054836	11.938637	-0.050786	4.815607
243.749339	8000.054193	11.943642	-0.050791	4.815607
243.823287	8000.024445	11.948647	-0.050805	4.815598
243.802141	8000.000624	11.953651	-0.050801	4.815591
244.028671	8000.007526	11.958656	-0.050844	4.815592
243.893145	7999.953014	11.963661	-0.050819	4.815577
243.810003	7999.977302	11.968666	-0.050803	4.815584
243.954660	7999.985008	11.973671	-0.050830	4.815586
243.928488	7999.982460	11.978675	-0.050826	4.815585
243.983291	8000.018602	11.983680	-0.050836	4.815596
243.754972	8000.001020	11.988685	-0.050794	4.815592
243.812578	8000.007310	11.993690	-0.050805	4.815593
243.754606	7999.995703	11.998695	-0.050794	4.815590
243.742038	7999.998716	12.003699	-0.050792	4.815591
243.819347	8000.004258	12.008704	-0.050806	4.815592
243.871185	7999.944253	12.013709	-0.050816	4.815574
243.693914	7999.975551	12.018714	-0.050783	4.815584
243.776256	7999.957685	12.023719	-0.050799	4.815579
243.820232	7999.958414	12.028723	-0.050807	4.815579
243.845327	7999.994072	12.033728	-0.050812	4.815589
243.821303	7999.976611	12.038733	-0.050808	4.815584
243.909154	7999.986596	12.043738	-0.050824	4.815587
243.839077	8000.028181	12.048743	-0.050811	4.815599
243.826759	7999.967131	12.053747	-0.050809	4.815581
244.051511	8000.040207	12.058752	-0.050851	4.815601
243.875837	7999.996787	12.063757	-0.050819	4.815590
243.862098	7999.990171	12.068762	-0.050816	4.815588
243.974705	8000.037931	12.073767	-0.050837	4.815601
243.944723	8000.008627	12.078771	-0.050832	4.815593
243.899794	8000.020723	12.083776	-0.050824	4.815596
244.079690	7999.975614	12.088781	-0.050857	4.815582
244.136064	7999.981884	12.093786	-0.050868	4.815584
243.983055	8000.012509	12.098791	-0.050840	4.815594
243.953518	7999.968263	12.103795	-0.050834	4.815581
244.107670	8000.025242	12.108800	-0.050863	4.815597
243.922356	7999.989139	12.113805	-0.050829	4.815587
243.937927	7999.991542	12.118810	-0.050832	4.815588
243.897589	8000.001577	12.123815	-0.050825	4.815591
243.919855	7999.962446	12.128819	-0.050829	4.815579
244.007568	8000.004462	12.133824	-0.050845	4.815591
243.740456	7999.955284	12.138829	-0.050796	4.815578
243.990519	7999.990331	12.143834	-0.050842	4.815587
244.136714	8000.022622	12.148839	-0.050870	4.815596
243.971433	8000.011404	12.153843	-0.050839	4.815593
244.091107	8000.016568	12.158848	-0.050862	4.815594
243.865385	7999.960588	12.163853	-0.050820	4.815579
244.126462	7999.992612	12.168858	-0.050869	4.815587
244.034195	8000.003938	12.173863	-0.050852	4.815591
243.956617	7999.980266	12.178867	-0.050837	4.815584
244.320060	8000.009685	12.183872	-0.050905	4.815591
244.076379	7999.972632	12.188877	-0.050860	4.815582
244.104015	7999.993383	12.193882	-0.050865	4.815587
244.354938	7999.954769	12.198887	-0.050912	4.815575
244.085951	7999.962152	12.203891	-0.050862	4.815578
244.104658	8000.019062	12.208896	-0.050866	4.815595
244.204657	7999.964111	12.213901	-0.050885	4.815578
244.101463	7999.976326	12.218906	-0.050865	4.815582
244.002194	8000.019572	12.223911	-0.050847	4.815596
243.997720	7999.970395	12.228915	-0.050846	4.815581
244.055169	8000.014055	12.233920	-0.050857	4.815594
243.970319	7999.979587	12.238925	-0.050842	4.815584
244.037393	8000.005251	12.243930	-0.050854	4.815591
243.997872	7999.984334	12.248935	-0.050847	4.815585
243.783228	7999.974449	12.253939	-0.050807	4.815583
244.012367	8000.014495	12.258944	-0.050850	4.815594
244.138563	7999.982393	12.263949	-0.050874	4.815584
244.010972	8000.011296	12.268954	-0.050850	4.815593
244.054202	7999.970370	12.273959	-0.050858	4.815581
243.917278	7999.971360	12.278963	-0.050833	4.815582
244.402902	7999.995292	12.283968	-0.050924	4.815587
244.205982	7999.959000	12.288973	-0.050887	4.815577
244.262727	8000.001581	12.293978	-0.050898	4.815589
244.391086	7999.972717	12.298983	-0.050922	4.815580
244.012103	7999.954819	12.303987	-0.050852	4.815577
244.165214	7999.972273	12.308992	-0.050880	4.815581
244.228205	7999.966905	12.313997	-0.050892	4.815579
244.114977	8000.001381	12.319002	-0.050871	4.815590
244.172706	8000.009809	12.324007	-0.050882	4.815592
244.100035	7999.999030	12.329011	-0.050869	4.815589
244.145938	8000.017943	12.334016	-0.050877	4.815594
243.977281	7999.975705	12.339021	-0.050846	4.815583
244.116804	7999.998276	12.344026	-0.050872	4.815589
244.180214	8000.007864	12.349031	-0.050884	4.815591
244.241827	7999.999270	12.354035	-0.050896	4.815588
244.253730	8000.009088	12.359040	-0.050898	4.815591
244.100589	7999.979915	12.364045	-0.050870	4.815583
244.195140	7999.977196	12.369050	-0.050888	4.815582
244.076010	8000.036135	12.374055	-0.050866	4.815600
243.950286	7999.980714	12.379059	-0.050842	4.815584
244.087021	8000.006444	12.384064	-0.050868	4.815591
244.010633	7999.964640	12.389069	-0.050854	4.815579
244.053176	8000.000582	12.394074	-0.050862	4.815590
243.989512	7999.983543	12.399079	-0.050850	4.815585
244.100525	7999.977889	12.404083	-0.050871	4.815583
244.021406	7999.983022	12.409088	-0.050857	4.815585
244.028481	7999.950050	12.414093	-0.050858	4.815575
243.946233	7999.995708	12.419098	-0.050843	4.815589
244.022876	7999.989494	12.424103	-0.050857	4.815587
244.159158	7999.972505	12.429107	-0.050883	4.815581
244.141271	8000.035227	12.434112	-0.050880	4.815599
244.093213	7999.975731	12.439117	-0.050871	4.815582
244.246778	7999.998531	12.444122	-0.050900	4.815588
244.357204	8000.011020	12.449127	-0.050920	4.815591
244.290924	7999.992871	12.454131	-0.050908	4.815586
244.321023	8000.028611	12.459136	-0.050914	4.815596
244.125136	7999.996607	12.464141	-0.050878	4.815588
244.274079	8000.015061	12.469146	-0.050906	4.815593
244.418108	8000.015283	12.474151	-0.050933	4.815592
244.217416	8000.001353	12.479155	-0.050895	4.815589
244.255774	8000.042567	12.484160	-0.050903	4.815601
244.286382	7999.992893	12.489165	-0.050908	4.815586
244.280669	7999.998153	12.494170	-0.050908	4.815588
244.341733	7999.982076	12.499175	-0.050919	4.815583
244.406407	7999.974600	12.504179	-0.050931	4.815580
244.481659	8000.044177	12.509184	-0.050945	4.815600
244.431161	8000.000657	12.514189	-0.050936	4.815588
244.261651	8000.007522	12.519194	-0.050905	4.815591
244.526177	8000.011841	12.524199	-0.050954	4.815591
244.347641	8000.007882	12.529203	-0.050921	4.815590
244.485068	8000.015471	12.534208	-0.050947	4.815592
244.501847	7999.979453	12.539213	-0.050950	4.815581
244.152414	7999.991933	12.544218	-0.050885	4.815587
244.348391	8000.007949	12.549223	-0.050922	4.815590
244.281969	7999.985526	12.554227	-0.050910	4.815584
244.229862	8000.019929	12.559232	-0.050900	4.815594
244.115295	8000.025553	12.564237	-0.050879	4.815596
244.352472	7999.992054	12.569242	-0.050923	4.815586
244.401477	8000.015289	12.574247	-0.050933	4.815592
244.355305	7999.963297	12.579251	-0.050924	4.815577
244.513174	8000.043829	12.584256	-0.050954	4.815600
244.467605	7999.984372	12.589261	-0.050945	4.815583
244.340474	8000.001537	12.594266	-0.050922	4.815588
244.342265	8000.011191	12.599271	-0.050922	4.815591
244.229894	8000.025392	12.604275	-0.050902	4.815596
244.483935	8000.054100	12.609280	-0.050949	4.815603
244.324203	8000.014141	12.614285	-0.050919	4.815592
244.420262	7999.984752	12.619290	-0.050937	4.815583
244.482714	7999.998596	12.624295	-0.050949	4.815587
244.260840	7999.981118	12.629299	-0.050908	4.815583
244.562387	8000.022344	12.634304	-0.050964	4.815593
244.540657	7999.978225	12.639309	-0.050961	4.815581
244.409143	7999.997454	12.644314	-0.050936	4.815587
244.430107	8000.030910	12.649319	-0.050940	4.815596
244.459611	8000.019659	12.654323	-0.050946	4.815593
244.542507	8000.038106	12.659328	-0.050962	4.815598
244.409089	7999.995373	12.664333	-0.050937	4.815586
244.461695	8000.030412	12.669338	-0.050947	4.815596
244.435388	8000.051353	12.674343	-0.050942	4.815602
244.268703	8000.007011	12.679347	-0.050911	4.815590
244.336372	8000.042295	12.684352	-0.050924	4.815600
244.458320	8000.018666	12.689357	-0.050947	4.815593
244.461043	8000.024063	12.694362	-0.050947	4.815594
244.383799	8000.024956	12.699367	-0.050933	4.815595
244.392745	7999.981336	12.704371	-0.050935	4.815582
244.259447	8000.031502	12.709376	-0.050910	4.815597
244.228282	7999.995772	12.714381	-0.050905	4.815587
244.481500	8000.020194	12.719386	-0.050952	4.815593
244.536549	8000.038189	12.724391	-0.050962	4.815598
244.321864	7999.987726	12.729395	-0.050923	4.815584
244.445939	8000.067707	12.734400	-0.050946	4.815607
244.456719	8000.024117	12.739405	-0.050948	4.815594
244.295944	8000.012972	12.744410	-0.050918	4.815592
244.256587	7999.982447	12.749415	-0.050911	4.815583
244.349779	7999.986113	12.754419	-0.050929	4.815584
244.525038	8000.045572	12.759424	-0.050961	4.815600
244.620737	7999.999093	12.764429	-0.050979	4.815586
244.501578	7999.999303	12.769434	-0.050957	4.815587
244.459954	8000.047758	12.774439	-0.050950	4.815601
244.472085	8000.007393	12.779443	-0.050952	4.815589
244.378946	8000.035789	12.784448	-0.050935	4.815598
244.490712	8000.062181	12.789453	-0.050956	4.815605
244.336624	8000.026585	12.794458	-0.050927	4.815596
244.293495	8000.010948	12.799463	-0.050920	4.815591
244.467186	8000.016992	12.804467	-0.050952	4.815592
244.644564	8000.070079	12.809472	-0.050985	4.815607
244.364664	8000.029233	12.814477	-0.050933	4.815596
244.378487	7999.999573	12.819482	-0.050936	4.815587
244.619751	8000.048361	12.824487	-0.050981	4.815601
244.613904	8000.017313	12.829491	-0.050980	4.815592
244.486571	8000.039814	12.834496	-0.050957	4.815599
244.417514	7999.999196	12.839501	-0.050944	4.815587
244.481874	8000.006664	12.844506	-0.050956	4.815589
244.396965	8000.011702	12.849511	-0.050940	4.815591
244.460128	7999.994592	12.854515	-0.050952	4.815586
244.475722	8000.065334	12.859520	-0.050955	4.815606
244.302009	8000.015537	12.864525	-0.050923	4.815592
244.332800	8000.018188	12.869530	-0.050929	4.815593
244.583865	7999.998796	12.874535	-0.050976	4.815586
244.635748	7999.985773	12.879539	-0.050986	4.815582
244.606107	8000.038694	12.884544	-0.050980	4.815598
244.592184	8000.091871	12.889549	-0.050978	4.815613
244.649711	8000.053313	12.894554	-0.050989	4.815602
244.561901	8000.071118	12.899559	-0.050973	4.815607
244.459803	7999.994724	12.904563	-0.050954	4.815586
244.393557	8000.064134	12.909568	-0.050942	4.815606
244.383343	8000.075727	12.914573	-0.050940	4.815610
244.222740	8000.052839	12.919578	-0.050910	4.815604
244.606691	8000.150933	12.924583	-0.050982	4.815631
244.407088	8000.080426	12.929587	-0.050945	4.815611
244.524710	8000.072745	12.934592	-0.050967	4.815608
244.487475	7999.997407	12.939597	-0.050960	4.815586
244.437962	7999.994479	12.944602	-0.050951	4.815586
244.423896	7999.998535	12.949607	-0.050949	4.815587
244.275587	7999.981186	12.954611	-0.050921	4.815582
244.504767	8000.039387	12.959616	-0.050964	4.815598
244.481432	8000.057174	12.964621	-0.050960	4.815604
244.367930	8000.027578	12.969626	-0.050939	4.815596
244.451130	8000.041759	12.974631	-0.050954	4.815599
244.312311	8000.014954	12.979635	-0.050929	4.815592
244.271903	8000.067700	12.984640	-0.050921	4.815608
244.477117	8000.079596	12.989645	-0.050960	4.815610
244.621902	8000.073424	12.994650	-0.050987	4.815608
244.490433	8000.049942	12.999655	-0.050963	4.815601
244.416257	7999.990020	13.004659	-0.050949	4.815584
244.553939	8000.029647	13.009664	-0.050975	4.815595
244.438368	8000.029916	13.014669	-0.050953	4.815596
244.437524	8000.036323	13.019674	-0.050953	4.815598
244.373082	8000.032084	13.024679	-0.050941	4.815597
244.469773	8000.024062	13.029683	-0.050960	4.815594
244.349154	8000.014638	13.034688	-0.050937	4.815592
244.448809	8000.020545	13.039693	-0.050956	4.815593
244.444725	7999.994865	13.044698	-0.050955	4.815586
244.408153	8000.029521	13.049703	-0.050949	4.815596
244.529177	8000.022962	13.054707	-0.050971	4.815593
244.663917	8000.049728	13.059712	-0.050997	4.815601
244.684742	8000.032996	13.064717	-0.051001	4.815596
244.491674	8000.041613	13.069722	-0.050965	4.815599
244.773647	8000.023793	13.074727	-0.051018	4.815592
244.622127	7999.995713	13.079731	-0.050990	4.815585
244.538498	8000.046688	13.084736	-0.050974	4.815600
244.420135	8000.006335	13.089741	-0.050952	4.815589
244.580473	8000.002551	13.094746	-0.050982	4.815587
244.458312	8000.029407	13.099751	-0.050960	4.815596
244.352494	8000.005275	13.104755	-0.050940	4.815589
244.635273	8000.049400	13.109760	-0.050993	4.815601
244.553365	8000.095063	13.114765	-0.050978	4.815614
244.411482	8000.098107	13.119770	-0.050952	4.815616
244.633364	8000.138038	13.124775	-0.050993	4.815626
244.577323	8000.016478	13.129779	-0.050983	4.815591
244.524266	8000.105323	13.134784	-0.050973	4.815617
244.459356	8000.055161	13.139789	-0.050961	4.815603
244.486510	8000.049210	13.144794	-0.050966	4.815601
244.542416	8000.061880	13.149799	-0.050977	4.815605
244.209475	7999.988136	13.154803	-0.050915	4.815585
244.448894	8000.017674	13.159808	-0.050960	4.815592
244.591706	8000.028554	13.164813	-0.050987	4.815595
244.377407	8000.025080	13.169818	-0.050947	4.815595
244.629146	8000.000361	13.174823	-0.050994	4.815586
244.527976	8000.010473	13.179827	-0.050975	4.815590
244.565111	8000.027109	13.184832	-0.050982	4.815594
244.513434	7999.983570	13.189837	-0.050973	4.815582
244.531422	7999.976402	13.194842	-0.050976	4.815580
244.528165	7999.983837	13.199847	-0.050976	4.815582
244.539185	7999.991505	13.204851	-0.050978	4.815584
244.465679	8000.039441	13.209856	-0.050965	4.815598
244.604775	8000.019295	13.214861	-0.050991	4.815592
244.479425	8000.014065	13.219866	-0.050967	4.815591
244.668019	8000.028894	13.224871	-0.051003	4.815594
244.481908	8000.048302	13.229875	-0.050968	4.815601
244.471345	8000.054551	13.234880	-0.050966	4.815603
244.429301	8000.058151	13.239885	-0.050959	4.815604
244.531958	8000.014989	13.244890	-0.050978	4.815591
244.734050	8000.102648	13.249895	-0.051016	4.815616
244.688631	8000.030380	13.254899	-0.051008	4.815595
244.964572	8000.037021	13.259904	-0.051059	4.815595
244.766844	7999.984697	13.264909	-0.051022	4.815581
244.642198	7999.988021	13.269914	-0.050999	4.815582
244.612235	8000.013175	13.274919	-0.050994	4.815590
244.606728	8000.034455	13.279923	-0.050993	4.815596
244.803233	8000.056888	13.284928	-0.051030	4.815602
244.566633	8000.092559	13.289933	-0.050986	4.815613
244.707933	8000.019059	13.294938	-0.051012	4.815591
244.743081	8000.064492	13.299943	-0.051019	4.815604
244.470711	8000.013090	13.304947	-0.050968	4.815591
244.620237	8000.051842	13.309952	-0.050997	4.815601
244.829810	7999.993335	13.314957	-0.051036	4.815583
244.824573	8000.027433	13.319962	-0.051035	4.815593
244.831608	8000.073477	13.324967	-0.051036	4.815606
244.702077	8000.020128	13.329971	-0.051012	4.815592
244.705587	8000.047961	13.334976	-0.051013	4.815600
244.519722	8000.049221	13.339981	-0.050979	4.815601
244.750863	8000.011353	13.344986	-0.051022	4.815589
244.979126	8000.099439	13.349991	-0.051065	4.815613
244.792277	8000.000309	13.354995	-0.051030	4.815585
244.724980	8000.040871	13.360000	-0.051018	4.815597
244.888323	8000.054222	13.365005	-0.051048	4.815601
244.858989	8000.019589	13.370010	-0.051043	4.815591
244.797956	8000.036762	13.375015	-0.051032	4.815596
244.608196	7999.968551	13.380019	-0.050996	4.815577
244.656101	8000.036616	13.385024	-0.051006	4.815596
244.593077	8000.038807	13.390029	-0.050994	4.815597
244.817482	8000.016846	13.395034	-0.051036	4.815590
244.944603	8000.087269	13.400039	-0.051060	4.815610
244.706157	7999.991570	13.405043	-0.051015	4.815583
244.804581	8000.012407	13.410048	-0.051034	4.815589
244.833886	8000.027847	13.415053	-0.051040	4.815593
244.666206	8000.005911	13.420058	-0.051009	4.815587
244.755008	8000.043675	13.425063	-0.051025	4.815598
244.431783	8000.001055	13.430067	-0.050965	4.815587
244.744257	8000.041392	13.435072	-0.051024	4.815597
244.724750	7999.998376	13.440077	-0.051020	4.815585
244.650518	8000.014267	13.445082	-0.051006	4.815590
244.758807	8000.060891	13.450087	-0.051027	4.815603
244.785066	7999.988721	13.455091	-0.051032	4.815582
244.713480	8000.071926	13.460096	-0.051019	4.815606
244.648934	8000.127483	13.465101	-0.051007	4.815623
244.657562	8000.032603	13.470106	-0.051009	4.815595
244.551306	8000.006328	13.475111	-0.050989	4.815588
244.565570	7999.970269	13.480115	-0.050992	4.815577
244.854352	8000.028373	13.485120	-0.051046	4.815593
244.744698	8000.007381	13.490125	-0.051025	4.815587
244.643176	7999.990793	13.495130	-0.051007	4.815583
244.833255	8000.037681	13.500135	-0.051042	4.815596
244.638281	7999.976860	13.505139	-0.051006	4.815579
244.583383	8000.015489	13.510144	-0.050996	4.815591
244.927140	8000.047793	13.515149	-0.051060	4.815598
244.948732	8000.006514	13.520154	-0.051064	4.815586
245.030462	8000.103961	13.525159	-0.051080	4.815614
244.961652	8000.075092	13.530163	-0.051067	4.815606
245.102915	8000.057117	13.535168	-0.051093	4.815600
244.942829	8000.051321	13.540173	-0.051064	4.815599
244.740980	8000.016015	13.545178	-0.051026	4.815590
245.055843	8000.062799	13.550183	-0.051085	4.815602
244.971771	8000.008054	13.555187	-0.051070	4.815587
244.815869	8000.019411	13.560192	-0.051041	4.815591
244.791336	8000.027568	13.565197	-0.051036	4.815593
244.774774	7999.988871	13.570202	-0.051033	4.815582
245.002749	8000.047054	13.575207	-0.051076	4.815598
244.786103	8000.002965	13.580211	-0.051036	4.815586
245.082467	8000.035566	13.585216	-0.051091	4.815594
244.921489	8000.007332	13.590221	-0.051061	4.815587
244.899486	8000.003784	13.595226	-0.051057	4.815586
244.910678	8000.014658	13.600231	-0.051060	4.815589
244.983875	8000.027609	13.605235	-0.051074	4.815592
244.835094	8000.025201	13.610240	-0.051046	4.815592
244.793320	8000.056569	13.615245	-0.051038	4.815601
244.929557	8000.037444	13.620250	-0.051064	4.815595
244.782022	8000.015836	13.625255	-0.051037	4.815590
244.763050	8000.006998	13.630259	-0.051033	4.815587
244.966280	8000.046626	13.635264	-0.051071	4.815598
244.869729	8000.032254	13.640269	-0.051053	4.815594
244.797667	8000.049248	13.645274	-0.051040	4.815599
245.005107	8000.038757	13.650279	-0.051079	4.815595
245.030019	7999.992193	13.655283	-0.051084	4.815582
244.987197	8000.008594	13.660288	-0.051076	4.815587
245.003329	8000.045176	13.665293	-0.051079	4.815597
244.961435	8000.035966	13.670298	-0.051071	4.815595
244.886967	8000.066801	13.675303	-0.051058	4.815604
244.875143	8000.014300	13.680307	-0.051056	4.815589
244.953025	8000.065769	13.685312	-0.051070	4.815603
244.984733	8000.038536	13.690317	-0.051076	4.815595
244.839822	8000.015902	13.695322	-0.051050	4.815589
244.970939	8000.037271	13.700327	-0.051074	4.815595
244.823281	8000.006050	13.705331	-0.051047	4.815587
244.787484	8000.021498	13.710336	-0.051040	4.815591
244.812781	8000.014449	13.715341	-0.051045	4.815589
244.862987	8000.023823	13.720346	-0.051055	4.815592
244.874056	8000.069932	13.725351	-0.051057	4.815605
244.767340	8000.003073	13.730355	-0.051037	4.815586
244.854709	8000.046153	13.735360	-0.051054	4.815598
244.871844	8000.035768	13.740365	-0.051057	4.815595
244.950829	8000.018915	13.745370	-0.051072	4.815590
245.110535	8000.061038	13.750375	-0.051102	4.815601
245.062679	8000.033577	13.755379	-0.051093	4.815593
244.845375	8000.035392	13.760384	-0.051053	4.815595
244.845138	8000.048216	13.765389	-0.051053	4.815599
244.862681	7999.996193	13.770394	-0.051056	4.815583
245.203579	8000.051944	13.775399	-0.051120	4.815598
244.992842	8000.011153	13.780403	-0.051081	4.815587
244.881471	8000.054202	13.785408	-0.051060	4.815600
244.919594	8000.072989	13.790413	-0.051067	4.815606
244.905509	8000.022586	13.795418	-0.051065	4.815591
245.026747	8000.067286	13.800423	-0.051088	4.815603
244.886274	8000.026572	13.805427	-0.051062	4.815592
244.944680	8000.043554	13.810432	-0.051073	4.815597
245.002417	8000.034897	13.815437	-0.051084	4.815594
244.895974	8000.017161	13.820442	-0.051064	4.815589
245.014558	8000.034055	13.825447	-0.051086	4.815594
244.950587	7999.962552	13.830451	-0.051074	4.815573
244.927076	8000.023048	13.835456	-0.051070	4.815591
244.929122	8000.012417	13.840461	-0.051071	4.815588
244.818820	7999.989279	13.845466	-0.051050	4.815582
244.900789	8000.010915	13.850471	-0.051066	4.815587
244.870530	8000.008301	13.855475	-0.051060	4.815587
244.941836	8000.029764	13.860480	-0.051074	4.815593
244.990030	8000.045512	13.865485	-0.051083	4.815597
244.901584	8000.005644	13.870490	-0.051067	4.815586
244.994952	8000.033873	13.875495	-0.051084	4.815594
244.848659	8000.001607	13.880499	-0.051057	4.815585
244.882272	8000.036338	13.885504	-0.051063	4.815595
244.992507	8000.036011	13.890509	-0.051084	4.815594
244.962368	7999.991753	13.895514	-0.051079	4.815582
245.117759	8000.024196	13.900519	-0.051108	4.815590
245.085453	8000.045040	13.905523	-0.051102	4.815596
245.072491	8000.018147	13.910528	-0.051100	4.815589
245.086513	7999.991694	13.915533	-0.051102	4.815581
245.027026	8000.008892	13.920538	-0.051091	4.815586
245.031059	8000.029260	13.925543	-0.051092	4.815592
244.810910	8000.012876	13.930547	-0.051052	4.815588
244.736031	8000.034095	13.935552	-0.051038	4.815595
245.192056	8000.011634	13.940557	-0.051123	4.815586
245.143718	8000.032217	13.945562	-0.051114	4.815592
245.072285	8000.041746	13.950567	-0.051101	4.815596
244.996313	8000.015963	13.955571	-0.051087	4.815588
244.999466	8000.033113	13.960576	-0.051088	4.815593
244.858997	8000.028705	13.965581	-0.051062	4.815593
244.911618	8000.014626	13.970586	-0.051072	4.815588
245.163757	8000.032626	13.975591	-0.051119	4.815592
245.096055	7999.986690	13.980595	-0.051106	4.815579
244.979482	8000.018976	13.985600	-0.051085	4.815589
244.995206	8000.059822	13.990605	-0.051088	4.815601
244.955187	8000.008997	13.995610	-0.051080	4.815587
244.953236	8000.039946	14.000615	-0.051080	4.815596
244.971737	8000.035990	14.005619	-0.051084	4.815594
244.945905	8000.040922	14.010624	-0.051079	4.815596
244.956499	8000.065668	14.015629	-0.051081	4.815603
244.940757	8000.062222	14.020634	-0.051079	4.815602
244.878377	8000.082576	14.025639	-0.051067	4.815608
244.954477	7999.999472	14.030643	-0.051081	4.815584
244.908825	8000.015828	14.035648	-0.051073	4.815589
245.121494	8000.001151	14.040653	-0.051113	4.815583
245.021679	8000.013421	14.045658	-0.051094	4.815587
245.025854	8000.023113	14.050663	-0.051095	4.815590
244.835154	7999.976243	14.055667	-0.051060	4.815577
244.906692	8000.013726	14.060672	-0.051073	4.815588
245.307858	8000.028814	14.065677	-0.051148	4.815591
244.921188	8000.028939	14.070682	-0.051077	4.815592
244.990043	8000.062108	14.075687	-0.051090	4.815602
245.037375	8000.016977	14.080691	-0.051098	4.815588
245.004841	8000.035681	14.085696	-0.051093	4.815594
245.089538	8000.033871	14.090701	-0.051108	4.815593
245.232283	8000.041548	14.095706	-0.051135	4.815595
245.075927	8000.047558	14.100711	-0.051106	4.815597
244.911761	8000.024611	14.105715	-0.051076	4.815591
245.058728	8000.068662	14.110720	-0.051103	4.815603
244.951013	8000.055176	14.115725	-0.051084	4.815600
244.893722	7999.991257	14.120730	-0.051073	4.815582
245.202091	8000.036868	14.125735	-0.051131	4.815593
245.220391	8000.075621	14.130739	-0.051134	4.815605
245.061636	8000.048490	14.135744	-0.051105	4.815597
245.127714	8000.074139	14.140749	-0.051117	4.815605
245.128240	8000.018635	14.145754	-0.051117	4.815588
245.263201	8000.064627	14.150759	-0.051143	4.815601
245.106536	8000.084514	14.155763	-0.051114	4.815608
245.084922	8000.082040	14.160768	-0.051110	4.815607
245.007677	8000.082932	14.165773	-0.051096	4.815608
245.110820	8000.057930	14.170778	-0.051115	4.815600
245.128494	8000.140454	14.175783	-0.051119	4.815624
245.065459	8000.086050	14.180787	-0.051107	4.815608
244.968046	8000.070596	14.185792	-0.051089	4.815604
245.091028	8000.073680	14.190797	-0.051112	4.815605
244.958444	8000.024551	14.195802	-0.051087	4.815591
245.140193	8000.041406	14.200807	-0.051121	4.815595
244.832610	8000.035344	14.205811	-0.051064	4.815595
245.035731	7999.185504	14.210816	-0.051102	4.815345

245.182295	7996.013753	14.215821	-0.051127	4.814417
245.009689	7990.550292	14.220826	-0.051092	4.812820
245.011766	7983.913724	14.225831	-0.051088	4.810878
245.012618	7976.668826	14.230835	-0.051083	4.808757
245.147838	7968.998631	14.235840	-0.051104	4.806510
245.062701	7961.216744	14.240845	-0.051083	4.804231
244.920182	7953.354668	14.245850	-0.051051	4.801926
244.957718	7945.367153	14.250855	-0.051053	4.799584
244.869709	7937.440184	14.255859	-0.051032	4.797258
244.752482	7929.402911	14.260864	-0.051005	4.794899
244.643578	7921.450530	14.265869	-0.050980	4.792564
244.662732	7913.318013	14.270874	-0.050978	4.790174
244.690352	7905.431726	14.275879	-0.050978	4.787855
244.609954	7897.381172	14.280883	-0.050958	4.785488
244.602829	7889.428970	14.285888	-0.050952	4.783147
244.451650	7881.436335	14.290893	-0.050919	4.780795
244.411079	7873.406782	14.295898	-0.050906	4.778429
244.509687	7865.388336	14.300903	-0.050919	4.776066
244.507788	7857.372540	14.305907	-0.050914	4.773702
244.419198	7849.379730	14.310912	-0.050892	4.771344
244.423556	7841.387839	14.315917	-0.050888	4.768985
244.463959	7833.411977	14.320922	-0.050891	4.766630
244.521347	7825.351518	14.325927	-0.050896	4.764248
244.199940	7817.423623	14.330931	-0.050831	4.761906
244.088099	7809.374508	14.335936	-0.050806	4.759525
244.083604	7801.397155	14.340941	-0.050800	4.757165
244.153011	7793.405629	14.345946	-0.050808	4.754799
244.082799	7785.341698	14.350951	-0.050789	4.752410
243.883731	7777.296252	14.355955	-0.050747	4.750027
243.999196	7769.326718	14.360960	-0.050764	4.747663
243.975284	7761.335452	14.365965	-0.050754	4.745293
244.092101	7753.346493	14.370970	-0.050771	4.742921
244.070819	7745.322257	14.375975	-0.050762	4.740539
243.912162	7737.347984	14.380979	-0.050727	4.738170
243.868019	7729.335830	14.385984	-0.050714	4.735788
243.835419	7721.319445	14.390989	-0.050703	4.733404
243.761190	7713.295192	14.395994	-0.050684	4.731017
243.737587	7705.320573	14.400999	-0.050674	4.728643
243.533002	7697.316918	14.406003	-0.050631	4.726260
243.568159	7689.327866	14.411008	-0.050633	4.723879
243.544677	7681.310928	14.416013	-0.050623	4.721489
243.597242	7673.273592	14.421018	-0.050628	4.719091
243.598397	7665.343442	14.426023	-0.050623	4.716724
243.532622	7657.314310	14.431027	-0.050606	4.714327
243.519522	7649.325227	14.436032	-0.050598	4.711940
243.285208	7641.312419	14.441037	-0.050550	4.709545
243.272429	7633.268897	14.446042	-0.050542	4.707140
243.391247	7625.277390	14.451047	-0.050559	4.704749
243.358924	7617.308657	14.456051	-0.050548	4.702363
243.111873	7609.274789	14.461056	-0.050497	4.699957
243.345203	7601.343102	14.466061	-0.050536	4.697580
243.055779	7593.304762	14.471066	-0.050477	4.695170
242.967754	7585.300017	14.476071	-0.050455	4.692769
243.038991	7577.279575	14.481075	-0.050463	4.690362
243.106933	7569.302710	14.486080	-0.050471	4.687966
243.206949	7561.300998	14.491085	-0.050485	4.685562
243.228278	7553.295665	14.496090	-0.050484	4.683156
243.338743	7545.317748	14.501095	-0.050499	4.680756
243.216573	7537.285656	14.506099	-0.050471	4.678339
242.964403	7529.306897	14.511104	-0.050419	4.675937
243.002049	7521.258062	14.516109	-0.050421	4.673513
242.702675	7513.120747	14.521114	-0.050360	4.671061
242.885411	7505.227973	14.526119	-0.050389	4.668681
243.031391	7497.230382	14.531123	-0.050411	4.666268
242.874462	7489.226388	14.536128	-0.050377	4.663852
242.681256	7481.257478	14.541133	-0.050336	4.661445
242.739194	7473.212050	14.546138	-0.050342	4.659014
242.818479	7465.287540	14.551143	-0.050352	4.656618
242.641063	7457.201180	14.556147	-0.050314	4.654173
242.501762	7449.183202	14.561152	-0.050282	4.651746
242.595514	7441.159804	14.566157	-0.050295	4.649317
242.599112	7433.227911	14.571162	-0.050291	4.646914
242.557681	7425.249566	14.576167	-0.050278	4.644495
242.153282	7417.275640	14.581171	-0.050197	4.642077
242.158240	7409.201924	14.586176	-0.050193	4.639628
242.111651	7401.282486	14.591181	-0.050180	4.637223
242.148546	7393.216265	14.596186	-0.050181	4.634773
242.204733	7385.206708	14.601191	-0.050187	4.632339
242.100039	7377.159068	14.606195	-0.050162	4.629892
242.027274	7369.195786	14.611200	-0.050144	4.627469
242.035901	7361.196786	14.616205	-0.050140	4.625034
241.995103	7353.224520	14.621210	-0.050128	4.622606
241.871282	7345.155025	14.626215	-0.050099	4.620148
241.818515	7337.189203	14.631219	-0.050084	4.617719
241.763662	7329.190764	14.636224	-0.050069	4.615279
241.771708	7321.223164	14.641229	-0.050066	4.612847
241.709014	7313.144295	14.646234	-0.050049	4.610380
241.742663	7305.182104	14.651239	-0.050050	4.607948
241.685998	7297.154749	14.656243	-0.050035	4.605494
241.636506	7289.166392	14.661248	-0.050020	4.603051
241.733055	7281.204579	14.666253	-0.050033	4.600614
241.560370	7273.173911	14.671258	-0.049996	4.598155
241.722089	7265.192958	14.676263	-0.050021	4.595710
241.598299	7257.159658	14.681267	-0.049993	4.593248
241.676058	7249.094719	14.686272	-0.050002	4.590775
241.644990	7241.142155	14.691277	-0.049991	4.588335
241.204954	7233.110392	14.696282	-0.049904	4.585869
241.496591	7225.144316	14.701287	-0.049954	4.583422
241.266629	7217.115738	14.706291	-0.049906	4.580954
241.209642	7209.120523	14.711296	-0.049890	4.578496
241.238263	7201.164878	14.716301	-0.049890	4.576048
241.205340	7193.150823	14.721306	-0.049879	4.573581
241.042702	7185.116226	14.726311	-0.049844	4.571106
241.044433	7177.096595	14.731315	-0.049839	4.568635
241.105743	7169.120560	14.736320	-0.049846	4.566176
241.104243	7161.148048	14.741325	-0.049840	4.563716
240.849152	7153.128331	14.746330	-0.049788	4.561240
240.941024	7145.163086	14.751335	-0.049800	4.558781
241.035397	7137.171799	14.756339	-0.049812	4.556311
241.023686	7129.137877	14.761344	-0.049805	4.553827
240.965897	7121.109589	14.766349	-0.049789	4.551344
240.806433	7113.111452	14.771354	-0.049754	4.548868
240.844551	7105.144897	14.776359	-0.049756	4.546401
240.543204	7097.106988	14.781363	-0.049695	4.543910
240.625650	7089.117710	14.786368	-0.049706	4.541433
240.585523	7081.118403	14.791373	-0.049693	4.538952
240.447373	7073.116053	14.796378	-0.049662	4.536468
240.478045	7065.106019	14.801383	-0.049663	4.533981
240.346301	7057.114499	14.806387	-0.049633	4.531498
240.254504	7049.079962	14.811392	-0.049611	4.529000
240.363013	7041.136816	14.816397	-0.049626	4.526529
240.592272	7033.080777	14.821402	-0.049664	4.524023
240.513910	7025.144636	14.826407	-0.049644	4.521551
240.389591	7017.082985	14.831411	-0.049616	4.519039
240.457532	7009.128519	14.836416	-0.049624	4.516560
240.287971	7001.133247	14.841421	-0.049587	4.514066
240.071192	6993.020838	14.846426	-0.049542	4.511533
240.064639	6985.017286	14.851431	-0.049535	4.509034
239.920680	6977.065300	14.856435	-0.049504	4.506549
239.892773	6969.032890	14.861440	-0.049493	4.504038
239.890626	6961.080588	14.866445	-0.049488	4.501551
239.885389	6953.052932	14.871450	-0.049482	4.499039
239.846145	6945.100855	14.876455	-0.049469	4.496549
239.817609	6937.068427	14.881459	-0.049459	4.494032
239.992859	6929.061453	14.886464	-0.049487	4.491523
239.969193	6921.059854	14.891469	-0.049477	4.489013
239.784074	6913.063372	14.896474	-0.049438	4.486503
239.635989	6905.055164	14.901479	-0.049405	4.483988
239.604323	6897.100966	14.906483	-0.049394	4.481488
239.512825	6889.055554	14.911488	-0.049372	4.478959
239.668520	6881.119227	14.916493	-0.049396	4.476463
239.478739	6873.040328	14.921498	-0.049355	4.473920
239.593000	6865.033076	14.926503	-0.049372	4.471399
239.390438	6856.990324	14.931507	-0.049329	4.468864
239.348600	6849.000853	14.936512	-0.049316	4.466346
239.437067	6841.005475	14.941517	-0.049327	4.463824
239.222785	6833.047878	14.946522	-0.049283	4.461312
239.404343	6825.057426	14.951527	-0.049311	4.458789
239.333740	6817.052815	14.956531	-0.049293	4.456260
239.382291	6809.001929	14.961536	-0.049297	4.453715
239.256740	6801.000278	14.966541	-0.049269	4.451183
239.293222	6793.007058	14.971546	-0.049270	4.448653
239.266111	6785.038924	14.976551	-0.049260	4.446130
239.151102	6777.034148	14.981555	-0.049234	4.443593
239.103120	6769.003559	14.986560	-0.049220	4.441046
239.183351	6761.040779	14.991565	-0.049230	4.438521
238.913386	6753.011663	14.996570	-0.049174	4.435971
238.872984	6745.008609	15.001575	-0.049162	4.433429
238.873200	6736.980125	15.006579	-0.049157	4.430878
238.787057	6728.984026	15.011584	-0.049136	4.428335
238.848583	6720.968812	15.016589	-0.049142	4.425785
238.912387	6712.968952	15.021594	-0.049149	4.423239
238.913307	6705.001085	15.026599	-0.049144	4.420701
238.804938	6697.008130	15.031603	-0.049119	4.418153
238.708966	6688.983431	15.036608	-0.049096	4.415594
238.745211	6681.005381	15.041613	-0.049098	4.413048
238.501417	6672.931757	15.046618	-0.049047	4.410469
238.535545	6664.997244	15.051623	-0.049048	4.407935
238.475341	6656.978007	15.056627	-0.049032	4.405372
238.337752	6649.017439	15.061632	-0.049001	4.402825
238.262828	6641.019533	15.066637	-0.048982	4.400265
238.349498	6633.036275	15.071642	-0.048994	4.397710
238.325755	6624.981572	15.076647	-0.048984	4.395129
238.149429	6616.995579	15.081651	-0.048946	4.392568
238.103543	6608.927398	15.086656	-0.048933	4.389980
238.355941	6601.004628	15.091661	-0.048975	4.387438
238.227989	6592.932751	15.096666	-0.048946	4.384846
238.053523	6585.014186	15.101671	-0.048908	4.382300
238.067412	6576.986210	15.106675	-0.048906	4.379719
238.179431	6569.035872	15.111680	-0.048921	4.377162
238.178143	6561.025340	15.116685	-0.048916	4.374584
238.024181	6552.967165	15.121690	-0.048882	4.371988
237.973428	6544.957410	15.126695	-0.048868	4.369406
237.783771	6537.015083	15.131699	-0.048828	4.366844
237.767718	6528.963871	15.136704	-0.048819	4.364246
237.888119	6521.028880	15.141709	-0.048837	4.361685
237.789413	6512.999447	15.146714	-0.048813	4.359091
237.756452	6505.071058	15.151719	-0.048802	4.356528
237.845569	6496.949966	15.156723	-0.048814	4.353902
237.661927	6488.875929	15.161728	-0.048774	4.351288
237.481075	6480.895443	15.166733	-0.048736	4.348703
237.557343	6472.934695	15.171738	-0.048745	4.346124
237.687493	6464.939016	15.176743	-0.048764	4.343532
237.436356	6456.986885	15.181747	-0.048712	4.340951
237.346258	6448.983282	15.186752	-0.048690	4.338353
237.144000	6441.010948	15.191757	-0.048648	4.335762
237.194094	6432.916034	15.196762	-0.048652	4.333132
237.261098	6424.952349	15.201767	-0.048659	4.330543
237.142581	6416.954330	15.206771	-0.048632	4.327940
237.089680	6408.914662	15.211776	-0.048617	4.325322
237.121316	6401.003503	15.216781	-0.048618	4.322745
237.238934	6392.942868	15.221786	-0.048635	4.320118
237.298750	6385.019514	15.226791	-0.048641	4.317535
237.067214	6376.968916	15.231795	-0.048593	4.314906
236.893114	6368.893320	15.236800	-0.048555	4.312267
237.062519	6360.879662	15.241805	-0.048582	4.309650
236.900147	6352.926366	15.246810	-0.048547	4.307048
236.869371	6344.905176	15.251815	-0.048536	4.304424
236.721564	6336.967023	15.256819	-0.048503	4.301824
236.766119	6328.912840	15.261824	-0.048507	4.299187
236.951902	6320.942997	15.266829	-0.048536	4.296576
236.724693	6312.958568	15.271834	-0.048489	4.293956
236.746410	6304.879744	15.276839	-0.048488	4.291305
236.682952	6296.914492	15.281843	-0.048471	4.288689
236.713903	6288.907114	15.286848	-0.048472	4.286058
236.615905	6280.944937	15.291853	-0.048448	4.283440
236.603016	6272.910551	15.296858	-0.048441	4.280797
236.605393	6264.915830	15.301863	-0.048436	4.278165
236.529772	6256.952693	15.306867	-0.048417	4.275542
236.551997	6248.885863	15.311872	-0.048416	4.272883
236.532000	6240.891411	15.316877	-0.048407	4.270247
236.259123	6232.855644	15.321882	-0.048351	4.267593
236.377555	6224.876938	15.326887	-0.048368	4.264959
236.319029	6216.909765	15.331891	-0.048352	4.262327
236.273149	6208.907552	15.336896	-0.048339	4.259681
236.158194	6200.977320	15.341901	-0.048312	4.257056
236.106015	6192.903219	15.346906	-0.048298	4.254383
236.076310	6184.905213	15.351911	-0.048287	4.251734
235.963628	6176.864611	15.356915	-0.048261	4.249068
236.008913	6168.923497	15.361920	-0.048264	4.246435
236.044017	6160.897295	15.366925	-0.048266	4.243772
235.736218	6152.921587	15.371930	-0.048204	4.241121
235.602932	6144.906553	15.376935	-0.048174	4.238456
235.724465	6136.954990	15.381939	-0.048191	4.235814
235.578178	6128.889465	15.386944	-0.048159	4.233129
235.679613	6120.909082	15.391949	-0.048173	4.230474
235.615031	6112.913258	15.396954	-0.048156	4.227810
235.615357	6104.905606	15.401959	-0.048151	4.225141
235.524241	6096.945982	15.406963	-0.048129	4.222485
235.473279	6088.913520	15.411968	-0.048114	4.219804
235.712460	6080.986788	15.416973	-0.048154	4.217159
235.404855	6072.925558	15.421978	-0.048091	4.214463
235.650132	6064.941402	15.426983	-0.048132	4.211796
235.477833	6056.905089	15.431987	-0.048095	4.209105
235.322807	6048.963883	15.436992	-0.048061	4.206445
235.331535	6040.973296	15.441997	-0.048057	4.203768
235.339868	6032.923574	15.447002	-0.048054	4.201070
235.337888	6024.983561	15.452007	-0.048049	4.198406
235.287560	6016.942267	15.457011	-0.048034	4.195707
235.249562	6008.858392	15.462016	-0.048022	4.192991
235.212066	6000.826192	15.467021	-0.048010	4.190291
235.042236	5992.862860	15.472026	-0.047973	4.187611
234.986068	5984.888025	15.477031	-0.047958	4.184927
235.169192	5976.899394	15.482035	-0.047987	4.182239
234.903930	5968.888891	15.487040	-0.047932	4.179537
234.872911	5960.944436	15.492045	-0.047921	4.176858
234.900248	5952.906952	15.497050	-0.047921	4.174146
234.918203	5944.899961	15.502055	-0.047920	4.171443
234.931991	5936.901071	15.507059	-0.047917	4.168741
234.798012	5928.881903	15.512064	-0.047887	4.166029
234.952009	5920.936643	15.517069	-0.047911	4.163343
234.690521	5912.880668	15.522074	-0.047857	4.160613
234.658962	5904.941044	15.527079	-0.047846	4.157923
234.712729	5896.949295	15.532083	-0.047851	4.155215
234.681140	5888.846084	15.537088	-0.047840	4.152467
234.747363	5880.873580	15.542093	-0.047847	4.149762
234.497516	5872.882456	15.547098	-0.047796	4.147045
234.579735	5864.875743	15.552103	-0.047806	4.144325
234.386974	5856.906989	15.557107	-0.047765	4.141613
234.262498	5848.875060	15.562112	-0.047737	4.138879
234.292478	5840.935517	15.567117	-0.047738	4.136176
234.221518	5832.875656	15.572122	-0.047719	4.133429
234.215109	5824.846303	15.577127	-0.047713	4.130691
234.157102	5816.902839	15.582131	-0.047697	4.127980
234.031696	5808.882084	15.587136	-0.047669	4.125240
234.121296	5800.944647	15.592141	-0.047680	4.122530
234.041095	5792.875374	15.597146	-0.047660	4.119770
234.120553	5784.968896	15.602151	-0.047670	4.117066
234.232568	5776.892223	15.607155	-0.047686	4.114303
233.973923	5768.817605	15.612160	-0.047633	4.111534
233.966933	5760.879219	15.617165	-0.047626	4.108813
233.827561	5752.896552	15.622170	-0.047595	4.106073
233.945304	5744.904884	15.627175	-0.047612	4.103332
233.824607	5736.908611	15.632179	-0.047585	4.100584
233.704650	5728.917726	15.637184	-0.047557	4.097836
233.562740	5720.926759	15.642189	-0.047526	4.095085
233.513345	5712.903152	15.647194	-0.047512	4.092323
233.704178	5704.860152	15.652199	-0.047542	4.089556
233.578575	5696.948211	15.657203	-0.047514	4.086828
233.371655	5688.908180	15.662208	-0.047470	4.084052
233.538604	5680.967338	15.667213	-0.047496	4.081314
233.336727	5672.923615	15.672218	-0.047453	4.078534
233.418834	5664.978810	15.677223	-0.047464	4.075790
233.566924	5656.924746	15.682227	-0.047486	4.073007
233.380172	5648.886124	15.687232	-0.047446	4.070222
233.262294	5640.944915	15.692237	-0.047419	4.067471
233.131483	5632.911488	15.697242	-0.047390	4.064685
233.223534	5624.940154	15.702247	-0.047402	4.061923
233.231419	5616.943516	15.707251	-0.047398	4.059148
233.125923	5608.945379	15.712256	-0.047374	4.056370
233.135781	5600.961427	15.717261	-0.047371	4.053596
233.082427	5592.901221	15.722266	-0.047355	4.050793
232.932844	5584.924234	15.727271	-0.047323	4.048015
232.997368	5576.935655	15.732275	-0.047330	4.045234
232.866035	5568.946550	15.737280	-0.047300	4.042449
232.860030	5560.929012	15.742285	-0.047294	4.039654
232.705315	5552.973512	15.747290	-0.047260	4.036876
232.791487	5544.922886	15.752295	-0.047271	4.034066
232.778286	5536.820509	15.757299	-0.047263	4.031235
232.655040	5528.856273	15.762304	-0.047235	4.028449
232.593980	5520.924324	15.767309	-0.047219	4.025673
232.551852	5512.920387	15.772314	-0.047206	4.022870
232.367917	5504.930087	15.777319	-0.047167	4.020067
232.622127	5496.953631	15.782323	-0.047209	4.017275
232.495189	5488.883939	15.787328	-0.047180	4.014442
232.490986	5480.898077	15.792333	-0.047175	4.011638
232.231356	5472.872419	15.797338	-0.047121	4.008814
232.301642	5464.906900	15.802343	-0.047129	4.006014
232.306873	5456.949870	15.807347	-0.047125	4.003215
232.184632	5448.930634	15.812352	-0.047097	4.000389
232.265100	5440.960129	15.817357	-0.047107	3.997582
232.332707	5432.921432	15.822362	-0.047115	3.994749
232.128767	5424.898264	15.827367	-0.047072	3.991915
232.182187	5416.878712	15.832371	-0.047077	3.989084
232.124387	5408.891198	15.837376	-0.047061	3.986261
232.190593	5400.945959	15.842381	-0.047068	3.983453
232.120015	5392.904218	15.847386	-0.047050	3.980606
232.065514	5384.924799	15.852391	-0.047035	3.977780
232.024321	5376.953096	15.857395	-0.047022	3.974954
231.848301	5368.916904	15.862400	-0.046984	3.972102
231.992932	5360.893295	15.867405	-0.047006	3.969257
231.717560	5352.919179	15.872410	-0.046950	3.966421
231.754212	5344.959634	15.877415	-0.046951	3.963593
231.614302	5336.980916	15.882419	-0.046920	3.960753
231.501567	5328.977732	15.887424	-0.046894	3.957903
231.763373	5320.971824	15.892429	-0.046938	3.955056
231.549348	5312.895816	15.897434	-0.046893	3.952174
231.546063	5304.916988	15.902439	-0.046887	3.949329
231.535811	5296.974867	15.907443	-0.046880	3.946494
231.314527	5288.937027	15.912448	-0.046834	3.943619
231.499599	5280.990677	15.917453	-0.046864	3.940782
231.472655	5273.004676	15.922458	-0.046854	3.937925
231.417926	5264.948279	15.927463	-0.046838	3.935041
231.332214	5257.001306	15.932467	-0.046817	3.932192
231.339961	5248.931807	15.937472	-0.046814	3.929300
231.261692	5240.991782	15.942477	-0.046794	3.926450
231.089997	5232.962322	15.947482	-0.046757	3.923564
231.042952	5225.015902	15.952487	-0.046743	3.920709
230.974536	5217.045139	15.957491	-0.046725	3.917842
230.863034	5209.011327	15.962496	-0.046700	3.914949
230.953835	5201.007768	15.967501	-0.046711	3.912069
230.810592	5192.971057	15.972506	-0.046680	3.909171
230.724611	5185.010971	15.977511	-0.046659	3.906299
230.833358	5176.999949	15.982515	-0.046674	3.903410
230.710183	5168.970634	15.987520	-0.046646	3.900508
230.924244	5160.997896	15.992525	-0.046681	3.897631
230.758861	5152.991383	15.997530	-0.046645	3.894732
230.432470	5144.990788	16.002535	-0.046579	3.891830
230.501585	5136.977929	16.007539	-0.046587	3.888929
230.400762	5128.984370	16.012544	-0.046563	3.886030
230.653940	5120.995994	16.017549	-0.046605	3.883137
230.497692	5113.007037	16.022554	-0.046571	3.880234
230.268808	5105.052092	16.027559	-0.046523	3.877339
230.269855	5097.025543	16.032563	-0.046518	3.874421
230.315518	5088.752172	16.037568	-0.046522	3.871412
230.400329	5080.843064	16.042573	-0.046532	3.868534
230.168709	5072.898835	16.047578	-0.046484	3.865634
230.207891	5064.950126	16.052583	-0.046487	3.862737
230.187665	5056.931106	16.057587	-0.046478	3.859810
230.014520	5048.964211	16.062592	-0.046440	3.856897
229.903856	5041.020453	16.067597	-0.046415	3.853991
229.894507	5033.000325	16.072602	-0.046408	3.851057
230.014486	5024.991051	16.077607	-0.046425	3.848128
229.744665	5017.018140	16.082611	-0.046370	3.845202
229.754709	5009.011035	16.087616	-0.046367	3.842266
229.794672	5001.026229	16.092621	-0.046369	3.839337
229.643025	4993.054928	16.097626	-0.046336	3.836407
229.718719	4985.003864	16.102631	-0.046345	3.833451
229.698704	4977.044200	16.107635	-0.046336	3.830523
229.538635	4969.039269	16.112640	-0.046301	3.827574
229.605765	4961.047064	16.117645	-0.046309	3.824632
229.739044	4953.055492	16.122650	-0.046329	3.821689
229.484975	4945.072893	16.127655	-0.046276	3.818739
229.328840	4937.081616	16.132659	-0.046242	3.815785
229.347021	4929.055230	16.137664	-0.046240	3.812820
229.570338	4921.057748	16.142669	-0.046277	3.809868
229.445166	4913.074924	16.147674	-0.046249	3.806912
229.347687	4905.084098	16.152679	-0.046225	3.803950
229.339252	4897.124621	16.157683	-0.046219	3.801001
229.069316	4889.109350	16.162688	-0.046163	3.798022
229.232780	4881.086608	16.167693	-0.046189	3.795047
229.120795	4873.071326	16.172698	-0.046163	3.792068
229.087315	4865.014072	16.177703	-0.046152	3.789071
229.082002	4857.090699	16.182707	-0.046146	3.786123
229.120300	4849.042659	16.187712	-0.046148	3.783127
229.181641	4841.110141	16.192717	-0.046154	3.780173
229.031270	4833.111228	16.197722	-0.046121	3.777186
228.900070	4825.121733	16.202727	-0.046092	3.774201
228.890532	4817.102826	16.207731	-0.046085	3.771206
228.789364	4809.035779	16.212736	-0.046061	3.768188
228.791489	4801.075700	16.217741	-0.046056	3.765210
228.634709	4793.104162	16.222746	-0.046022	3.762221
228.515182	4785.110092	16.227751	-0.045995	3.759223
228.564760	4777.147805	16.232755	-0.045999	3.756238
228.490664	4769.108025	16.237760	-0.045980	3.753219
228.556965	4761.098437	16.242765	-0.045987	3.750211
228.320330	4753.090045	16.247770	-0.045938	3.747195
228.333891	4745.065942	16.252775	-0.045935	3.744177
228.349778	4737.126072	16.257779	-0.045933	3.741187
228.212475	4729.135926	16.262784	-0.045903	3.738173
228.253053	4721.162588	16.267789	-0.045905	3.735167
228.098302	4713.142697	16.272794	-0.045871	3.732136
228.278073	4705.116431	16.277799	-0.045900	3.729108
228.144904	4697.135511	16.282803	-0.045870	3.726088
228.063896	4689.147075	16.287808	-0.045850	3.723063
228.087356	4681.169198	16.292813	-0.045849	3.720043
227.820363	4673.211507	16.297818	-0.045794	3.717020
227.816446	4665.166128	16.302823	-0.045789	3.713968
227.872287	4657.068431	16.307827	-0.045794	3.710896
227.785261	4649.085246	16.312832	-0.045773	3.707861
227.697351	4641.130038	16.317837	-0.045751	3.704833
227.800991	4633.148389	16.322842	-0.045766	3.701799
227.607679	4625.202492	16.327847	-0.045725	3.698767
227.618957	4617.224404	16.332851	-0.045722	3.695727
227.592178	4609.191582	16.337856	-0.045712	3.692661
227.555761	4601.217575	16.342861	-0.045700	3.689616
227.459353	4593.197793	16.347866	-0.045677	3.686549
227.346500	4585.220911	16.352871	-0.045651	3.683495
227.455294	4577.226168	16.357875	-0.045666	3.680438
227.664988	4569.228849	16.362880	-0.045700	3.677379
227.582145	4561.247906	16.367885	-0.045679	3.674317
227.416349	4553.217419	16.372890	-0.045643	3.671232
227.382153	4545.230409	16.377895	-0.045632	3.668163
227.469634	4537.232146	16.382899	-0.045643	3.665091
227.347661	4529.270960	16.387904	-0.045615	3.662025
227.517740	4521.259388	16.392909	-0.045642	3.658945
227.122537	4513.270304	16.397914	-0.045563	3.655856
227.213522	4505.251722	16.402919	-0.045575	3.652766
227.256561	4497.218919	16.407923	-0.045578	3.649667
227.107080	4489.242495	16.412928	-0.045545	3.646581
227.001678	4481.262596	16.417933	-0.045521	3.643493
226.814805	4473.273368	16.422938	-0.045481	3.640396
226.935809	4465.285822	16.427943	-0.045498	3.637306
227.006109	4457.256210	16.432947	-0.045506	3.634195
226.966237	4449.229054	16.437952	-0.045494	3.631080
226.864799	4441.276598	16.442957	-0.045470	3.627989
226.827200	4433.251021	16.447962	-0.045458	3.624869
226.736243	4425.290677	16.452967	-0.045436	3.621770
226.721221	4417.311806	16.457971	-0.045428	3.618663
226.468398	4409.310137	16.462976	-0.045376	3.615538
226.815094	4401.294669	16.467981	-0.045435	3.612422
226.479335	4393.283243	16.472986	-0.045368	3.609285
226.493853	4385.322702	16.477991	-0.045366	3.606176
226.394024	4377.359629	16.482995	-0.045342	3.603060
226.202916	4369.367764	16.488000	-0.045301	3.599927
226.355739	4361.406071	16.493005	-0.045325	3.596812
226.466987	4353.346739	16.498010	-0.045340	3.593656
226.421503	4345.335972	16.503015	-0.045327	3.590512
226.185961	4337.374604	16.508019	-0.045278	3.587378
226.158913	4329.351193	16.513024	-0.045268	3.584224
226.116899	4321.419240	16.518029	-0.045255	3.581102
226.015774	4313.407396	16.523034	-0.045231	3.577945
226.045259	4305.407380	16.528039	-0.045231	3.574793
225.998454	4297.392315	16.533043	-0.045218	3.571630
225.814520	4289.364419	16.538048	-0.045178	3.568455
225.750403	4281.407580	16.543053	-0.045161	3.565309
225.667482	4273.441829	16.548058	-0.045141	3.562156
225.606898	4265.456293	16.553063	-0.045125	3.558993
225.774441	4257.465670	16.558067	-0.045151	3.555832
225.617212	4249.337869	16.563072	-0.045116	3.552604
225.950902	4241.310601	16.568077	-0.045173	3.549428
225.753431	4233.370191	16.573082	-0.045132	3.546268
225.850654	4225.373244	16.578087	-0.045145	3.543091
225.872665	4217.412613	16.583091	-0.045144	3.539923
225.530792	4209.463832	16.588096	-0.045075	3.536746
225.717162	4201.438575	16.593101	-0.045105	3.533552
225.752852	4193.402205	16.598106	-0.045106	3.530346
225.632199	4185.438133	16.603111	-0.045079	3.527162
225.340635	4177.494337	16.608115	-0.045019	3.523977
225.386631	4169.500098	16.613120	-0.045023	3.520779
225.468937	4161.528245	16.618125	-0.045033	3.517589
225.371135	4153.502693	16.623130	-0.045010	3.514368
225.308902	4145.479476	16.628135	-0.044993	3.511147
225.361328	4137.474232	16.633139	-0.044998	3.507934
225.159603	4129.506833	16.638144	-0.044955	3.504725
225.172099	4121.532542	16.643149	-0.044953	3.501516
225.137150	4113.535929	16.648154	-0.044941	3.498295
225.088526	4105.539254	16.653159	-0.044927	3.495070
225.017342	4097.588099	16.658163	-0.044909	3.491859
224.978744	4089.541292	16.663168	-0.044896	3.488609
225.068267	4081.566057	16.668173	-0.044908	3.485388
224.852392	4073.606772	16.673178	-0.044863	3.482160
224.641625	4065.602941	16.678183	-0.044819	3.478912
224.753707	4057.611941	16.683187	-0.044834	3.475677
224.648314	4049.569441	16.688192	-0.044810	3.472410
224.590964	4041.558404	16.693197	-0.044794	3.469155
224.743616	4033.578101	16.698202	-0.044817	3.465916
224.622385	4025.599460	16.703207	-0.044790	3.462665
224.638764	4017.608925	16.708211	-0.044788	3.459412
224.481121	4009.629155	16.713216	-0.044753	3.456153
224.564896	4001.597032	16.718221	-0.044764	3.452879
224.571174	3993.595554	16.723226	-0.044760	3.449611
224.375138	3985.619541	16.728231	-0.044718	3.446344
224.452769	3977.658751	16.733235	-0.044728	3.443089
224.135714	3969.655237	16.738240	-0.044664	3.439800
224.073515	3961.727068	16.743245	-0.044647	3.436548
223.972534	3953.659045	16.748250	-0.044623	3.433233
224.048733	3945.613237	16.753255	-0.044632	3.429931
224.089290	3937.653203	16.758259	-0.044635	3.426659
224.068453	3929.673958	16.763264	-0.044626	3.423375
224.314242	3921.700872	16.768269	-0.044667	3.420098
223.970839	3913.747646	16.773274	-0.044598	3.416807
223.872292	3905.717720	16.778279	-0.044574	3.413489
224.058720	3897.690889	16.783283	-0.044604	3.410179
223.873106	3889.708745	16.788288	-0.044564	3.406872
223.648392	3881.715088	16.793293	-0.044517	3.403555
223.775870	3873.771449	16.798298	-0.044536	3.400268
223.800889	3865.774802	16.803303	-0.044536	3.396952
223.781968	3857.764840	16.808307	-0.044527	3.393626
223.525409	3849.707651	16.813312	-0.044474	3.390269
223.520429	3841.734120	16.818317	-0.044468	3.386951
223.288552	3833.780838	16.823322	-0.044420	3.383631
223.478294	3825.772809	16.828327	-0.044450	3.380300
223.567531	3817.811787	16.833331	-0.044462	3.376982
223.349825	3809.799494	16.838336	-0.044416	3.373628
223.198942	3801.804505	16.843341	-0.044383	3.370280
223.090418	3793.833301	16.848346	-0.044358	3.366941
223.207147	3785.839590	16.853351	-0.044375	3.363596
223.242337	3777.863756	16.858355	-0.044376	3.360253
222.903956	3769.867777	16.863360	-0.044308	3.356885
223.078216	3761.866964	16.868365	-0.044336	3.353530
223.206580	3753.849854	16.873370	-0.044354	3.350163
223.006761	3745.869180	16.878375	-0.044312	3.346796
222.889813	3737.894623	16.883379	-0.044285	3.343431
223.079396	3729.879287	16.888384	-0.044316	3.340056
222.798600	3721.943288	16.893389	-0.044258	3.336695
222.693362	3713.938805	16.898394	-0.044234	3.333308
222.628397	3705.924974	16.903399	-0.044216	3.329914
222.726769	3697.944050	16.908403	-0.044230	3.326538
222.495928	3689.956735	16.913408	-0.044182	3.323142
222.662643	3681.970575	16.918413	-0.044208	3.319759
222.575321	3674.004649	16.923418	-0.044186	3.316371
222.502580	3665.959776	16.928423	-0.044168	3.312947
222.558527	3657.951414	16.933427	-0.044173	3.309540
222.428603	3649.971472	16.938432	-0.044144	3.306134
222.340618	3642.007782	16.943437	-0.044122	3.302733
222.329229	3634.001657	16.948442	-0.044115	3.299314
222.494312	3626.025267	16.953447	-0.044141	3.295910
222.550897	3618.044172	16.958451	-0.044146	3.292497
222.227392	3610.034855	16.963456	-0.044081	3.289053
222.440342	3602.057777	16.968461	-0.044116	3.285641
222.414675	3594.088631	16.973466	-0.044106	3.282219
222.250741	3586.102568	16.978471	-0.044070	3.278780
222.123687	3578.148457	16.983475	-0.044042	3.275354
221.990451	3570.096784	16.988480	-0.044012	3.271881
221.840480	3562.118222	16.993485	-0.043979	3.268436
221.862097	3554.090551	16.998490	-0.043978	3.264972
221.857266	3546.141704	17.003495	-0.043972	3.261538
222.032723	3538.135648	17.008499	-0.043999	3.258082
221.728235	3530.156861	17.013504	-0.043938	3.254616
221.603236	3522.184604	17.018509	-0.043909	3.251156
221.606847	3514.166602	17.023514	-0.043905	3.247677
221.512047	3506.166289	17.028519	-0.043882	3.244199
221.716478	3498.212914	17.033523	-0.043915	3.240749
221.414912	3490.230284	17.038528	-0.043854	3.237262
221.602738	3482.223059	17.043533	-0.043884	3.233781
221.472491	3474.178189	17.048538	-0.043855	3.230267
221.419991	3466.188471	17.053543	-0.043840	3.226776
221.312569	3458.231842	17.058547	-0.043815	3.223293
221.123737	3450.270824	17.063552	-0.043775	3.219801
221.140261	3442.283569	17.068557	-0.043773	3.216303
221.140990	3434.273048	17.073562	-0.043768	3.212790
221.156364	3426.240063	17.078567	-0.043766	3.209263
221.081730	3418.301791	17.083571	-0.043747	3.205771
221.111433	3410.314103	17.088576	-0.043747	3.202257
221.062318	3402.360361	17.093581	-0.043733	3.198752
220.908778	3394.353837	17.098586	-0.043699	3.195215
220.994264	3386.334178	17.103591	-0.043710	3.191678
221.150336	3378.334983	17.108595	-0.043734	3.188149
221.094728	3370.312647	17.113600	-0.043719	3.184597
220.851917	3362.414455	17.118605	-0.043669	3.181088
220.762039	3354.415411	17.123610	-0.043647	3.177537
220.840035	3346.417625	17.128615	-0.043656	3.173990
220.777925	3338.419095	17.133619	-0.043640	3.170432
220.659357	3330.428021	17.138624	-0.043612	3.166872
220.752248	3322.448627	17.143629	-0.043625	3.163321
220.731143	3314.478718	17.148634	-0.043616	3.159766
220.610671	3306.507887	17.153639	-0.043588	3.156203
220.599235	3298.507570	17.158643	-0.043581	3.152626
220.533210	3290.467280	17.163648	-0.043564	3.149026
220.485342	3282.479022	17.168653	-0.043550	3.145445
220.295401	3274.543034	17.173658	-0.043509	3.141878
220.256287	3266.538799	17.178663	-0.043497	3.138282
220.306949	3258.558523	17.183667	-0.043501	3.134697
220.105388	3250.544280	17.188672	-0.043459	3.131081
220.203658	3242.554786	17.193677	-0.043472	3.127486
220.222966	3234.565649	17.198682	-0.043471	3.123883
220.078973	3226.615737	17.203687	-0.043439	3.120287
220.174947	3218.668470	17.208691	-0.043452	3.116698
220.055570	3210.646976	17.213696	-0.043424	3.113062
219.788989	3202.661309	17.218701	-0.043370	3.109431
219.757015	3194.682972	17.223706	-0.043359	3.105810
219.710273	3186.694830	17.228711	-0.043345	3.102179
219.809982	3178.683531	17.233715	-0.043358	3.098540
219.702843	3170.690741	17.238720	-0.043333	3.094896
219.781999	3162.720825	17.243725	-0.043343	3.091267
219.589320	3154.728871	17.248730	-0.043302	3.087611
219.536429	3146.723469	17.253735	-0.043287	3.083951
219.736997	3138.758532	17.258739	-0.043320	3.080316
219.493125	3130.796916	17.263744	-0.043269	3.076659
219.431095	3122.760398	17.268749	-0.043253	3.072971
219.581607	3114.703070	17.273754	-0.043275	3.069279
219.493095	3106.747642	17.278759	-0.043254	3.065618
219.380687	3098.808277	17.283763	-0.043228	3.061959
219.418124	3090.804191	17.288768	-0.043230	3.058273
219.564819	3082.834368	17.293773	-0.043252	3.054603
219.185699	3074.890979	17.298778	-0.043177	3.050916
219.190345	3066.876681	17.303783	-0.043172	3.047210
219.226974	3058.893764	17.308787	-0.043174	3.043516
219.182086	3050.914820	17.313792	-0.043161	3.039815
219.226528	3042.990141	17.318797	-0.043164	3.036139
219.001672	3034.984823	17.323802	-0.043117	3.032409
218.881092	3026.962533	17.328807	-0.043090	3.028670
218.947966	3018.976223	17.333811	-0.043097	3.024953
218.736531	3011.013365	17.338816	-0.043053	3.021229
218.757488	3003.039470	17.343821	-0.043051	3.017506
218.935189	2995.020945	17.348826	-0.043079	3.013766
218.692756	2987.022401	17.353831	-0.043029	3.010010
218.666277	2979.075822	17.358835	-0.043019	3.006283
218.623212	2971.077702	17.363840	-0.043006	3.002528
218.483718	2963.152244	17.368845	-0.042975	2.998797
218.547736	2955.150877	17.373850	-0.042982	2.995035
218.549827	2947.103172	17.378855	-0.042977	2.991244
218.361628	2939.155982	17.383859	-0.042937	2.987486
218.249410	2931.147390	17.388864	-0.042911	2.983698
218.272078	2923.186123	17.393869	-0.042911	2.979935
218.222776	2915.210953	17.398874	-0.042896	2.976156
218.049063	2907.211856	17.403879	-0.042859	2.972355
218.151658	2899.236868	17.408883	-0.042873	2.968575
218.009153	2891.235924	17.413888	-0.042841	2.964765
218.034945	2883.295431	17.418893	-0.042841	2.960987
217.881852	2875.318193	17.423898	-0.042808	2.957178
217.951887	2867.297165	17.428903	-0.042816	2.953354
217.903372	2859.306483	17.433907	-0.042802	2.949534
217.918166	2851.327152	17.438912	-0.042799	2.945718
217.952287	2843.349544	17.443917	-0.042801	2.941898
217.899517	2835.369603	17.448922	-0.042786	2.938068
217.641873	2827.420446	17.453927	-0.042733	2.934237
217.812430	2819.407220	17.458931	-0.042759	2.930393
217.525924	2811.440736	17.463936	-0.042701	2.926542
217.530088	2803.466675	17.468941	-0.042697	2.922697
217.555303	2795.496272	17.473946	-0.042696	2.918851
217.439907	2787.512435	17.478951	-0.042670	2.914985
217.412762	2779.441888	17.483955	-0.042660	2.911077
217.353645	2771.448794	17.488960	-0.042644	2.907199
217.556429	2763.464483	17.493965	-0.042676	2.903335
217.426373	2755.544833	17.498970	-0.042647	2.899479
217.259589	2747.571899	17.503975	-0.042611	2.895590
217.391692	2739.564438	17.508979	-0.042631	2.891695
217.197185	2731.593130	17.513984	-0.042589	2.887795
217.081081	2723.639289	17.518989	-0.042563	2.883902
217.058327	2715.683924	17.523994	-0.042553	2.880008
217.045145	2707.680953	17.528999	-0.042546	2.876086
217.285835	2699.667485	17.534003	-0.042586	2.872168
216.758031	2691.719234	17.539008	-0.042482	2.868234
216.969795	2683.706720	17.544013	-0.042517	2.864303
216.921633	2675.779927	17.549018	-0.042503	2.860396
216.802671	2667.804305	17.554023	-0.042476	2.856454
216.806344	2659.820857	17.559027	-0.042471	2.852511
216.649852	2651.826829	17.564032	-0.042437	2.848547
216.738215	2643.816274	17.569037	-0.042448	2.844584
216.766768	2635.880222	17.574042	-0.042449	2.840649
216.606385	2627.920105	17.579047	-0.042414	2.836685
216.646243	2619.920179	17.584051	-0.042416	2.832708
216.444984	2611.901977	17.589056	-0.042374	2.828702
216.382611	2603.926279	17.594061	-0.042357	2.824720
216.472130	2595.951973	17.599066	-0.042369	2.820741
216.348070	2587.988407	17.604071	-0.042341	2.816750
216.263765	2580.028516	17.609075	-0.042320	2.812757
216.345406	2571.992487	17.614080	-0.042330	2.808730
216.251728	2564.030979	17.619085	-0.042307	2.804724
216.164578	2556.105562	17.624090	-0.042286	2.800732
216.021012	2548.138577	17.629095	-0.042254	2.796709
215.852805	2540.145799	17.634099	-0.042218	2.792666
215.834111	2532.138086	17.639104	-0.042210	2.788618
216.050282	2524.131370	17.644109	-0.042245	2.784579
215.893298	2516.202963	17.649114	-0.042211	2.780552
215.671655	2508.245105	17.654119	-0.042164	2.776500
215.619127	2500.255919	17.659123	-0.042149	2.772436
215.709203	2492.227479	17.664128	-0.042161	2.768354
215.543693	2484.272585	17.669133	-0.042125	2.764289
215.606253	2476.321057	17.674138	-0.042132	2.760233
215.720356	2468.344005	17.679143	-0.042148	2.756162
215.685362	2460.307884	17.684147	-0.042136	2.752045
215.310846	2452.329312	17.689152	-0.042062	2.747931
215.309537	2444.361949	17.694157	-0.042056	2.743839
215.523906	2436.368828	17.699162	-0.042091	2.739740
215.173460	2428.444170	17.704167	-0.042021	2.735637
215.242363	2420.454620	17.709171	-0.042029	2.731519
215.291052	2412.454120	17.714176	-0.042033	2.727388
215.247929	2404.509799	17.719181	-0.042020	2.723275
215.169463	2396.566068	17.724186	-0.042000	2.719153
215.166147	2388.573759	17.729191	-0.041994	2.715005
215.243864	2380.588170	17.734195	-0.042004	2.710858
214.796056	2372.636382	17.739200	-0.041915	2.706690
214.944876	2364.665569	17.744205	-0.041938	2.702543
214.913914	2356.682520	17.749210	-0.041927	2.698372
214.905843	2348.686410	17.754215	-0.041921	2.694190
214.943384	2340.697218	17.759219	-0.041923	2.690007
214.810492	2332.734475	17.764224	-0.041893	2.685820
214.677810	2324.809127	17.769229	-0.041863	2.681647
214.620269	2316.845002	17.774234	-0.041847	2.677452
214.518176	2308.855006	17.779239	-0.041823	2.673233
214.602983	2300.842549	17.784243	-0.041834	2.669008
214.425040	2292.861742	17.789248	-0.041796	2.664777
214.440382	2284.920202	17.794253	-0.041794	2.660571
214.457676	2276.967446	17.799258	-0.041792	2.656353
214.448509	2268.940134	17.804263	-0.041785	2.652088
214.244341	2261.012056	17.809267	-0.041742	2.647855
214.054991	2253.034384	17.814272	-0.041702	2.643590
214.146224	2245.064417	17.819277	-0.041714	2.639341
214.119794	2237.126380	17.824282	-0.041704	2.635094
214.199284	2229.098408	17.829287	-0.041714	2.630799
214.216595	2221.140885	17.834291	-0.041712	2.626531
214.111835	2213.179454	17.839296	-0.041687	2.622245
214.027578	2205.213489	17.844301	-0.041667	2.617952
214.123119	2197.233123	17.849306	-0.041679	2.613655
214.066850	2189.227210	17.854311	-0.041664	2.609328
213.886152	2181.315254	17.859315	-0.041625	2.605036
213.560148	2173.383603	17.864320	-0.041559	2.600716
213.685074	2165.398105	17.869325	-0.041578	2.596390
213.598241	2157.307437	17.874330	-0.041556	2.591986
213.480499	2149.263938	17.879335	-0.041529	2.587597
213.627722	2141.334151	17.884339	-0.041552	2.583282
213.407390	2133.409460	17.889344	-0.041506	2.578936
213.343350	2125.449810	17.894349	-0.041489	2.574575
213.339105	2117.475665	17.899354	-0.041483	2.570203
213.131776	2109.522539	17.904359	-0.041439	2.565820
213.172304	2101.578160	17.909363	-0.041442	2.561453
213.198555	2093.618827	17.914368	-0.041442	2.557068
213.123056	2085.662009	17.919373	-0.041423	2.552670
213.071287	2077.684060	17.924378	-0.041408	2.548255
213.000797	2069.707143	17.929383	-0.041390	2.543831
213.042744	2061.761579	17.934387	-0.041393	2.539425
212.959472	2053.806185	17.939392	-0.041372	2.534996
212.899841	2045.821667	17.944397	-0.041356	2.530546
212.813485	2037.868064	17.949402	-0.041335	2.526103
212.960015	2029.874106	17.954407	-0.041357	2.521646
212.853232	2021.955660	17.959411	-0.041332	2.517205
212.717305	2013.969059	17.964416	-0.041302	2.512716
212.515543	2005.997229	17.969421	-0.041259	2.508223
212.708223	1998.018060	17.974426	-0.041290	2.503746
212.383460	1990.064784	17.979431	-0.041225	2.499238
212.578499	1982.111316	17.984435	-0.041256	2.494760
212.506626	1974.110096	17.989440	-0.041237	2.490227
212.276150	1966.179809	17.994445	-0.041189	2.485714
212.212060	1958.234216	17.999450	-0.041172	2.481197
212.213279	1950.270787	18.004455	-0.041168	2.476666
212.132346	1942.309367	18.009459	-0.041148	2.472122
212.070540	1934.325178	18.014464	-0.041131	2.467557
212.202250	1926.336514	18.019469	-0.041150	2.462997
212.135794	1918.415686	18.024474	-0.041133	2.458451
211.936401	1910.451729	18.029479	-0.041091	2.453863
212.055679	1902.478326	18.034483	-0.041108	2.449285
211.752845	1894.551129	18.039488	-0.041047	2.444692
212.003358	1886.564313	18.044493	-0.041088	2.440099
211.798372	1878.645112	18.049498	-0.041045	2.435501
211.745153	1870.580261	18.054503	-0.041030	2.430822
211.944599	1862.595308	18.059507	-0.041062	2.426200
211.557642	1854.682946	18.064512	-0.040985	2.421565
211.653581	1846.719826	18.069517	-0.040998	2.416930
211.654955	1838.768180	18.074522	-0.040993	2.412285
211.316574	1830.824777	18.079527	-0.040925	2.407610
211.589840	1822.837931	18.084531	-0.040971	2.402947
211.587399	1814.887496	18.089536	-0.040966	2.398276
211.510616	1806.934390	18.094541	-0.040946	2.393587
211.438136	1798.986814	18.099546	-0.040928	2.388894
211.372725	1791.006983	18.104551	-0.040911	2.384172
211.226400	1783.098343	18.109555	-0.040878	2.379477
211.123312	1775.138359	18.114560	-0.040854	2.374745
211.256121	1767.135038	18.119565	-0.040874	2.369997
211.350997	1759.176062	18.124570	-0.040886	2.365263
211.191472	1751.240086	18.129575	-0.040852	2.360513
211.233813	1743.309603	18.134579	-0.040855	2.355773
211.121280	1735.327269	18.139584	-0.040829	2.350979
210.940404	1727.383516	18.144589	-0.040790	2.346194
210.798352	1719.444336	18.149594	-0.040758	2.341404
210.767281	1711.473574	18.154599	-0.040748	2.336594
211.027453	1703.481429	18.159603	-0.040791	2.331786
210.832808	1695.542291	18.164608	-0.040750	2.326962
210.577190	1687.631904	18.169613	-0.040697	2.322141
210.850245	1679.656668	18.174618	-0.040743	2.317314
210.648587	1671.703667	18.179623	-0.040700	2.312451
210.640582	1663.744826	18.184627	-0.040694	2.307591
210.512275	1655.796823	18.189632	-0.040665	2.302716
210.361183	1647.884109	18.194637	-0.040632	2.297851
210.322753	1639.924029	18.199642	-0.040620	2.292956
210.180340	1631.949453	18.204647	-0.040588	2.288033
210.215299	1624.009349	18.209651	-0.040589	2.283135
210.055595	1616.079852	18.214656	-0.040555	2.278217
210.018272	1608.091531	18.219661	-0.040543	2.273263
210.102201	1600.067701	18.224666	-0.040553	2.268285
209.823413	1592.152790	18.229671	-0.040496	2.263334
209.940224	1584.210682	18.234675	-0.040513	2.258388
210.005001	1576.243240	18.239680	-0.040520	2.253412
209.962672	1568.285366	18.244685	-0.040507	2.248421
209.890701	1560.364702	18.249690	-0.040489	2.243440
209.716272	1552.435597	18.254695	-0.040451	2.238433
209.878160	1544.481262	18.259699	-0.040476	2.233429
209.721381	1536.531548	18.264704	-0.040442	2.228389
209.609087	1528.593432	18.269709	-0.040416	2.223348
209.748106	1520.642021	18.274714	-0.040437	2.218310
209.491022	1512.716255	18.279719	-0.040384	2.213241
209.429579	1504.770513	18.284723	-0.040368	2.208165
209.350708	1496.830167	18.289728	-0.040348	2.203079
209.241333	1488.911043	18.294733	-0.040323	2.197993
209.087518	1480.968064	18.299738	-0.040289	2.192875
209.008012	1472.980911	18.304743	-0.040269	2.187724
209.211684	1465.012074	18.309747	-0.040302	2.182598
208.927821	1457.106425	18.314752	-0.040244	2.177456
209.096917	1449.128569	18.319757	-0.040271	2.172297
209.223006	1441.170372	18.324762	-0.040289	2.167134
209.048370	1433.247816	18.329767	-0.040252	2.161955
209.036523	1425.338542	18.334771	-0.040244	2.156787
209.046984	1417.380747	18.339776	-0.040241	2.151576
208.934819	1409.446687	18.344781	-0.040215	2.146357
208.867594	1401.524837	18.349786	-0.040198	2.141138
208.782201	1393.576491	18.354791	-0.040177	2.135887
208.670721	1385.652662	18.359795	-0.040151	2.130636
208.553997	1377.726136	18.364800	-0.040125	2.125370
208.391893	1369.804745	18.369805	-0.040089	2.120090
208.346168	1361.885463	18.374810	-0.040076	2.114810
208.217965	1353.855273	18.379815	-0.040047	2.109434
208.242858	1345.913352	18.384819	-0.040047	2.104118
208.103849	1338.010322	18.389824	-0.040016	2.098799
208.206835	1330.054789	18.394829	-0.040030	2.093455
208.299687	1322.105232	18.399834	-0.040042	2.088100
208.041150	1314.201489	18.404839	-0.039989	2.082728
208.174642	1306.268819	18.409843	-0.040009	2.077361
208.000444	1298.352093	18.414848	-0.039971	2.071960
208.075018	1290.392592	18.419853	-0.039980	2.066541
208.149775	1282.459564	18.424858	-0.039989	2.061126
207.906014	1274.567082	18.429863	-0.039939	2.055692
207.885400	1266.640244	18.434867	-0.039930	2.050243
207.694761	1258.716436	18.439872	-0.039889	2.044764
207.889372	1250.773176	18.444877	-0.039921	2.039296
207.770988	1242.868066	18.449882	-0.039894	2.033808
207.642873	1234.895353	18.454887	-0.039865	2.028257
207.663541	1226.974069	18.459891	-0.039863	2.022741
207.493478	1219.069933	18.464896	-0.039827	2.017203
207.463766	1211.130127	18.469901	-0.039816	2.011640
207.519415	1203.195871	18.474906	-0.039822	2.006073
207.285011	1195.298463	18.479911	-0.039773	2.000487
207.276651	1187.392361	18.484915	-0.039766	1.994903
206.983237	1179.483402	18.489920	-0.039707	1.989271
206.969915	1171.542846	18.494925	-0.039699	1.983630
206.899199	1163.630132	18.499930	-0.039681	1.977986
206.948329	1155.683517	18.504935	-0.039685	1.972315
207.034532	1147.743704	18.509939	-0.039696	1.966637
206.923130	1139.838715	18.514944	-0.039671	1.960946
206.971164	1131.935446	18.519949	-0.039675	1.955257
206.978555	1123.960259	18.524954	-0.039671	1.949494
206.738586	1116.051142	18.529959	-0.039621	1.943736
206.717768	1108.152615	18.534963	-0.039612	1.937992
206.489533	1100.255703	18.539968	-0.039565	1.932210
206.649253	1092.291915	18.544973	-0.039590	1.926403
206.670823	1084.397474	18.549978	-0.039589	1.920615
206.320498	1076.531933	18.554983	-0.039518	1.914790
206.326355	1068.602050	18.559987	-0.039514	1.908938
206.414502	1060.671971	18.564992	-0.039526	1.903078
206.254118	1052.786703	18.569997	-0.039491	1.897205
206.203866	1044.869464	18.575002	-0.039477	1.891303
206.109650	1036.953390	18.580007	-0.039454	1.885377
206.103750	1029.070422	18.585011	-0.039448	1.879468
206.074241	1021.158810	18.590016	-0.039438	1.873517
206.046569	1013.216260	18.595021	-0.039427	1.867522
205.917401	1005.330776	18.600026	-0.039398	1.861541
205.815098	997.423490	18.605031	-0.039374	1.855526
205.837887	989.517403	18.610035	-0.039374	1.849507
205.769868	981.612786	18.615040	-0.039356	1.843459
205.819649	973.712170	18.620045	-0.039360	1.837408
205.652249	965.840713	18.625050	-0.039324	1.831334
205.553149	957.931245	18.630055	-0.039301	1.825218
205.609273	950.029832	18.635059	-0.039306	1.819107
205.649374	942.125260	18.640064	-0.039309	1.812970
205.585330	934.222692	18.645069	-0.039292	1.806802
205.626983	926.335148	18.650074	-0.039294	1.800637
205.277958	918.487429	18.655079	-0.039224	1.794435
205.237809	910.539269	18.660083	-0.039212	1.788170
205.159701	902.642792	18.665088	-0.039192	1.781918
205.063199	894.765910	18.670093	-0.039169	1.775658
205.139066	886.852421	18.675098	-0.039179	1.769369
205.107924	878.958280	18.680103	-0.039168	1.763058
205.163855	871.089479	18.685107	-0.039173	1.756757
204.997046	863.210035	18.690112	-0.039137	1.750396
204.856086	855.344106	18.695117	-0.039106	1.744026
204.746414	847.487485	18.700122	-0.039081	1.737644
204.562721	839.600145	18.705127	-0.039041	1.731204
204.657472	831.706939	18.710131	-0.039054	1.724771
204.529714	823.856546	18.715136	-0.039025	1.718320
204.311645	815.985342	18.720141	-0.038980	1.711816
204.330190	808.086914	18.725146	-0.038978	1.705296
204.232197	800.216717	18.730151	-0.038955	1.698759
204.417780	792.311454	18.735155	-0.038985	1.692204
204.374204	784.429380	18.740160	-0.038971	1.685613
204.025167	776.614986	18.745165	-0.038902	1.679013
204.305142	768.709843	18.750170	-0.038949	1.672394
204.060884	760.854759	18.755175	-0.038898	1.665720
203.958340	753.016153	18.760179	-0.038874	1.659053
203.863598	745.152836	18.765184	-0.038852	1.652339
203.699817	737.287913	18.770189	-0.038816	1.645586
203.754593	729.434648	18.775194	-0.038821	1.638846
203.654163	721.538516	18.780199	-0.038798	1.632020
203.702077	713.639690	18.785203	-0.038802	1.625183
203.550252	705.820644	18.790208	-0.038768	1.618358
203.507366	697.954632	18.795213	-0.038755	1.611479
203.482397	690.100490	18.800218	-0.038746	1.604584
203.274980	682.292236	18.805223	-0.038702	1.597673
203.441745	674.411794	18.810227	-0.038728	1.590722
203.207278	666.592143	18.815232	-0.038680	1.583736
203.256618	658.738910	18.820237	-0.038684	1.576731
203.218211	650.888248	18.825242	-0.038672	1.569684
203.029635	643.074949	18.830247	-0.038632	1.562617
203.076657	635.244032	18.835251	-0.038636	1.555536
203.016580	627.379486	18.840256	-0.038619	1.548376
202.967567	619.546093	18.845261	-0.038605	1.541214
202.862156	611.740935	18.850266	-0.038581	1.534035
202.783328	603.892863	18.855271	-0.038561	1.526787
202.594100	596.101204	18.860275	-0.038521	1.519540
202.462103	588.290845	18.865280	-0.038492	1.512250
202.448652	580.446767	18.870285	-0.038484	1.504910
202.357449	572.654070	18.875290	-0.038462	1.497571
202.136805	564.837504	18.880295	-0.038416	1.490154
202.137343	557.023652	18.885299	-0.038411	1.482736
202.016021	549.228464	18.890304	-0.038384	1.475279
202.004918	541.349760	18.895309	-0.038377	1.467722
202.135460	533.526395	18.900314	-0.038396	1.460202
201.887282	525.754572	18.905319	-0.038345	1.452632
202.202759	517.893413	18.910323	-0.038399	1.445026
201.922983	510.159968	18.915328	-0.038342	1.437408
201.679220	502.391591	18.920333	-0.038292	1.429722
201.792063	494.579843	18.925338	-0.038308	1.422009
201.716495	486.796166	18.930343	-0.038289	1.414251
201.612751	479.016124	18.935347	-0.038264	1.406450
201.511506	471.255486	18.940352	-0.038241	1.398624
201.500193	463.455675	18.945357	-0.038234	1.390730
201.590986	455.660279	18.950362	-0.038246	1.382813
201.259943	447.937012	18.955367	-0.038179	1.374852
201.176070	440.171967	18.960371	-0.038159	1.366844
201.258195	432.394219	18.965376	-0.038169	1.358805
201.256063	424.624916	18.970381	-0.038164	1.350711
201.013628	416.907587	18.975386	-0.038114	1.342582
200.872741	409.166846	18.980391	-0.038082	1.334396
200.892812	401.397484	18.985395	-0.038081	1.326157
200.816425	393.682987	18.990400	-0.038062	1.317908
200.644004	385.853820	18.995405	-0.038025	1.309467
200.728519	378.074289	19.000410	-0.038036	1.301071
200.393537	370.402233	19.005415	-0.037969	1.292661
200.411119	362.666512	19.010419	-0.037967	1.284192
200.410512	354.951886	19.015424	-0.037962	1.275685
200.200477	347.259130	19.020429	-0.037918	1.267107
200.119685	339.571711	19.025434	-0.037898	1.258501
200.188382	331.839367	19.030439	-0.037906	1.249813
200.053069	324.167853	19.035443	-0.037876	1.241094
199.991434	316.482568	19.040448	-0.037860	1.232312
199.869451	308.782631	19.045453	-0.037832	1.223439
199.911898	301.102349	19.050458	-0.037835	1.214555
199.701942	293.439157	19.055463	-0.037791	1.205576
199.552503	285.806531	19.060467	-0.037759	1.196578
199.478667	278.138137	19.065472	-0.037740	1.187484
199.501163	270.469385	19.070477	-0.037740	1.178339
199.389079	262.837743	19.075482	-0.037714	1.169140
199.299177	255.204526	19.080487	-0.037692	1.159871
199.203004	247.562997	19.085491	-0.037670	1.150515
199.152849	239.913866	19.090496	-0.037655	1.141083
198.965997	232.315327	19.095501	-0.037616	1.131606
198.991324	224.694796	19.100506	-0.037616	1.122067
198.830383	217.111081	19.105511	-0.037581	1.112452
198.784017	209.520706	19.110515	-0.037568	1.102770
198.900057	201.907321	19.115520	-0.037584	1.093009
198.585758	194.377705	19.120525	-0.037521	1.083172
198.550317	186.820966	19.125530	-0.037510	1.073273
198.228263	179.287842	19.130535	-0.037445	1.063247
198.119128	171.752886	19.135539	-0.037420	1.053172
198.176404	164.192145	19.140544	-0.037426	1.043004
198.016133	156.686618	19.145549	-0.037391	1.032760
198.127046	149.149416	19.150554	-0.037407	1.022434
198.044319	141.651968	19.155559	-0.037387	1.012012
197.738441	134.212732	19.160563	-0.037325	1.001508
197.666088	126.722846	19.165568	-0.037307	0.990879
197.683583	119.221663	19.170573	-0.037306	0.980141
197.647437	111.773052	19.175578	-0.037294	0.969346
197.249903	104.393857	19.180583	-0.037216	0.958439
197.320817	96.948618	19.185587	-0.037224	0.947431
197.199093	89.559924	19.190592	-0.037197	0.936327
197.036048	82.180849	19.195597	-0.037162	0.925093
196.743847	74.860684	19.200602	-0.037103	0.913777
196.696609	67.482268	19.205607	-0.037089	0.902296
196.623734	60.381165	19.210611	-0.037071	0.891098