Thu Mar 11 18:10:59 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.518107	0.115949	0.000000	0.000059	0.723603

0.600699	0.115392	0.005005	0.000043	0.723631
0.569546	0.124733	0.010010	0.000049	0.723639
0.483382	0.134310	0.015014	0.000065	0.723628
0.582584	0.086993	0.020019	0.000046	0.723570
0.687152	-0.047986	0.025024	0.000027	0.723342
0.553134	-0.028373	0.030029	0.000052	0.723334
0.654663	-0.041582	0.035034	0.000033	0.723344
0.620435	-0.039935	0.040038	0.000039	0.723336
0.500488	-0.015344	0.045043	0.000061	0.723342
0.573777	-0.030173	0.050048	0.000047	0.723339
0.545284	-0.026601	0.055053	0.000052	0.723336
0.596089	-0.033168	0.060058	0.000043	0.723341
0.456164	-0.010871	0.065062	0.000069	0.723337
0.490120	-0.013681	0.070067	0.000062	0.723343
0.454502	-0.009558	0.075072	0.000069	0.723339
0.305943	0.014993	0.080077	0.000096	0.723336
0.428155	-0.004606	0.085082	0.000073	0.723340
0.528638	-0.130623	0.090086	0.000054	0.723129
0.634095	-0.211781	0.095091	0.000035	0.723006
0.558254	-0.198824	0.100096	0.000049	0.723006
0.474507	-0.186448	0.105101	0.000064	0.723001
0.526604	-0.191694	0.110106	0.000054	0.723009
0.302028	-0.155994	0.115110	0.000096	0.723001
0.445395	-0.197226	0.120115	0.000069	0.722971
0.452576	-0.339308	0.125120	0.000068	0.722695
0.296716	-0.315045	0.130125	0.000096	0.722688
0.285127	-0.307761	0.135130	0.000098	0.722699
0.263875	-0.309057	0.140134	0.000102	0.722689
0.490513	-0.344667	0.145139	0.000060	0.722698
0.327201	-0.468703	0.150144	0.000090	0.722398
0.486746	-0.510895	0.155149	0.000060	0.722371
0.344453	-0.481970	0.160154	0.000087	0.722379
0.107368	-0.443878	0.165158	0.000131	0.722371
0.298983	-0.559828	0.170163	0.000095	0.722211
0.460524	-0.658007	0.175168	0.000065	0.722075
0.132960	-0.600822	0.180173	0.000126	0.722073
0.548493	-0.671583	0.185178	0.000048	0.722079
0.528236	-0.803642	0.190182	0.000052	0.721813
0.524872	-0.836397	0.195187	0.000052	0.721748
0.455485	-0.823991	0.200192	0.000065	0.721748
0.601132	-0.929979	0.205197	0.000038	0.721591
0.489173	-0.985037	0.210202	0.000059	0.721444
0.404729	-0.974714	0.215206	0.000074	0.721435
0.454140	-1.049043	0.220211	0.000065	0.721306
0.414422	-1.136499	0.225216	0.000072	0.721121
0.097230	-1.082823	0.230221	0.000131	0.721116
0.224606	-1.159381	0.235226	0.000107	0.721010
0.308413	-1.245033	0.240230	0.000091	0.720871
0.243700	-1.230999	0.245235	0.000103	0.720876
0.234025	-1.351430	0.250240	0.000105	0.720636
0.215749	-1.400469	0.255245	0.000108	0.720534
0.224160	-1.413931	0.260250	0.000107	0.720510
-0.086133	-1.506528	0.265254	0.000164	0.720220
0.083235	-1.533508	0.270259	0.000133	0.720226
0.242010	-1.646740	0.275264	0.000103	0.720059
-0.049043	-1.676041	0.280269	0.000157	0.719900
-0.000276	-1.693629	0.285274	0.000148	0.719882
0.118392	-1.858013	0.290278	0.000126	0.719600
0.141534	-1.860580	0.295283	0.000121	0.719604
0.020756	-1.971855	0.300288	0.000144	0.719342
-0.008667	-2.005990	0.305293	0.000149	0.719265
-0.327449	-2.029191	0.310298	0.000208	0.719107
-0.875885	-2.010483	0.315302	0.000310	0.718952
-1.668087	-1.868274	0.320307	0.000457	0.718954
-2.934471	-1.801210	0.325312	0.000693	0.718642
-3.358233	-1.725251	0.330317	0.000772	0.718643
-3.037615	-1.780209	0.335322	0.000712	0.718648
-3.525202	-1.773663	0.340326	0.000803	0.718490
-4.420187	-1.681889	0.345331	0.000969	0.718356
-3.860072	-1.783260	0.350336	0.000865	0.718353
-4.148913	-1.733505	0.355341	0.000918	0.718350
-4.380095	-1.792112	0.360346	0.000961	0.718154
-5.420173	-1.676670	0.365350	0.001155	0.718016
-5.002043	-1.750068	0.370355	0.001077	0.718018
-5.246683	-1.707116	0.375360	0.001122	0.718018
-5.247541	-1.721374	0.380365	0.001122	0.717989
-5.604403	-1.801378	0.385370	0.001188	0.717706
-6.166620	-1.705849	0.390374	0.001293	0.717697
-6.480535	-1.648662	0.395379	0.001351	0.717700
-5.860012	-1.758033	0.400384	0.001235	0.717703
-6.068973	-1.739442	0.405389	0.001274	0.717666
-6.877959	-1.739003	0.410394	0.001425	0.717382
-6.991531	-1.721804	0.415398	0.001446	0.717377
-6.981295	-1.721446	0.420403	0.001444	0.717381
-6.986134	-1.720022	0.425408	0.001444	0.717383
-7.119022	-1.700250	0.430413	0.001469	0.717375
-7.158985	-1.784446	0.435418	0.001476	0.717195
-8.187447	-1.659758	0.440422	0.001667	0.717079
-7.976912	-1.695829	0.445427	0.001628	0.717083
-7.776965	-1.730133	0.450432	0.001591	0.717085
-8.263170	-1.646912	0.455437	0.001681	0.717079
-8.180159	-1.657585	0.460442	0.001665	0.717087
-8.030172	-1.769503	0.465446	0.001637	0.716919
-8.994926	-1.680429	0.470451	0.001817	0.716756
-8.988367	-1.681193	0.475456	0.001816	0.716757
-9.350134	-1.619267	0.480461	0.001883	0.716752
-8.982814	-1.680113	0.485466	0.001814	0.716761
-8.899339	-1.701913	0.490470	0.001799	0.716748
-9.230254	-1.639054	0.495475	0.001860	0.716756
-9.155179	-1.781425	0.500480	0.001846	0.716501
-9.904282	-1.677383	0.505485	0.001985	0.716443
-9.914661	-1.672293	0.510490	0.001987	0.716450
-9.842005	-1.689680	0.515494	0.001973	0.716441
-9.771930	-1.699551	0.520499	0.001960	0.716447
-9.918271	-1.674026	0.525504	0.001987	0.716446
-10.172258	-1.666453	0.530509	0.002034	0.716372
-10.501573	-1.728600	0.535514	0.002095	0.716133
-10.544220	-1.724067	0.540518	0.002103	0.716127
-11.090474	-1.624426	0.545523	0.002205	0.716132
-10.560453	-1.717689	0.550528	0.002106	0.716134
-10.450810	-1.740166	0.555533	0.002085	0.716129
-10.525621	-1.724821	0.560538	0.002099	0.716133
-11.034799	-1.714473	0.565542	0.002194	0.715974
-11.577345	-1.665395	0.570547	0.002295	0.715880
-11.326643	-1.710519	0.575552	0.002248	0.715880
-11.589633	-1.666260	0.580557	0.002297	0.715875
-11.342393	-1.706434	0.585562	0.002250	0.715883
-11.352683	-1.709160	0.590566	0.002252	0.715874
-11.704960	-1.655376	0.595571	0.002318	0.715857
-12.084391	-1.744129	0.600576	0.002388	0.715547
-12.174908	-1.732679	0.605581	0.002405	0.715538
-12.425341	-1.683924	0.610586	0.002451	0.715546
-12.610225	-1.655230	0.615590	0.002486	0.715538
-12.330039	-1.701552	0.620595	0.002433	0.715546
-12.229468	-1.719144	0.625600	0.002414	0.715547
-12.662641	-1.696760	0.630605	0.002495	0.715438
-13.408256	-1.668522	0.635610	0.002634	0.715231
-13.388256	-1.676325	0.640614	0.002630	0.715223
-13.583326	-1.640739	0.645619	0.002666	0.715225
-13.329413	-1.684429	0.650624	0.002618	0.715228
-13.214153	-1.707904	0.655629	0.002597	0.715223
-13.288573	-1.690112	0.660634	0.002611	0.715232
-13.484769	-1.676123	0.665638	0.002647	0.715191
-14.116998	-1.707729	0.670643	0.002764	0.714905
-14.099915	-1.709111	0.675648	0.002761	0.714909
-14.792623	-1.589078	0.680653	0.002890	0.714902
-14.300967	-1.672764	0.685658	0.002798	0.714910
-14.298424	-1.678045	0.690662	0.002798	0.714901
-14.584462	-1.625348	0.695667	0.002851	0.714905
-14.450869	-1.648116	0.700672	0.002826	0.714907
-14.499662	-1.730093	0.705677	0.002835	0.714727
-15.181942	-1.668370	0.710682	0.002961	0.714609
-15.208434	-1.668712	0.715686	0.002966	0.714599
-15.324684	-1.643118	0.720691	0.002988	0.714609
-15.200562	-1.665694	0.725696	0.002964	0.714608
-15.519937	-1.611381	0.730701	0.003024	0.714604
-15.349192	-1.638568	0.735706	0.002992	0.714610
-15.159044	-1.725972	0.740710	0.002956	0.714504
-16.131557	-1.669419	0.745715	0.003137	0.714273
-15.891965	-1.710916	0.750720	0.003092	0.714275
-16.214357	-1.656339	0.755725	0.003152	0.714270
-16.066768	-1.678066	0.760730	0.003125	0.714279
-16.290109	-1.639642	0.765734	0.003166	0.714277
-16.347290	-1.628425	0.770739	0.003177	0.714279
-15.920536	-1.735171	0.775744	0.003097	0.714219
-17.267558	-1.624134	0.780749	0.003348	0.713963
-17.153351	-1.638936	0.785754	0.003326	0.713974
-17.004171	-1.668922	0.790758	0.003298	0.713968
-16.999931	-1.670650	0.795763	0.003297	0.713966
-16.989728	-1.670221	0.800768	0.003295	0.713971
-17.130392	-1.650138	0.805773	0.003321	0.713961
-16.857324	-1.693989	0.810778	0.003270	0.713971
-17.667773	-1.702251	0.815782	0.003421	0.713668
-18.357681	-1.588941	0.820787	0.003549	0.713649
-17.782260	-1.690118	0.825792	0.003442	0.713652
-18.137188	-1.630367	0.830797	0.003508	0.713645
-18.084127	-1.635926	0.835802	0.003498	0.713653
-17.856878	-1.680566	0.840806	0.003456	0.713645
-17.848805	-1.679758	0.845811	0.003454	0.713650
-18.248543	-1.688837	0.850816	0.003528	0.713491
-19.108984	-1.605100	0.855821	0.003688	0.713353
-18.462118	-1.715478	0.860826	0.003568	0.713363
-18.985730	-1.625826	0.865830	0.003665	0.713356
-19.431746	-1.546586	0.870835	0.003748	0.713356
-18.631908	-1.687045	0.875840	0.003599	0.713360
-19.001028	-1.623663	0.880845	0.003667	0.713356
-18.941711	-1.669026	0.885850	0.003656	0.713287
-19.629015	-1.681734	0.890854	0.003784	0.713018
-19.792439	-1.651509	0.895859	0.003814	0.713020
-20.027579	-1.610193	0.900864	0.003858	0.713020
-20.032715	-1.612877	0.905869	0.003859	0.713013
-19.631357	-1.679165	0.910874	0.003784	0.713023
-20.138458	-1.592215	0.915878	0.003878	0.713017
-20.222935	-1.577116	0.920883	0.003894	0.713017
-19.571748	-1.783482	0.925888	0.003772	0.712838
-21.073522	-1.585087	0.930893	0.004052	0.712700
-20.717918	-1.644206	0.935898	0.003985	0.712709
-20.884178	-1.616612	0.940902	0.004016	0.712705
-21.230153	-1.556800	0.945907	0.004080	0.712702
-20.615929	-1.662823	0.950912	0.003966	0.712709
-20.872549	-1.620540	0.955917	0.004013	0.712703
-20.695207	-1.696973	0.960922	0.003980	0.712614
-21.894575	-1.600121	0.965926	0.004203	0.712381
-21.993323	-1.581459	0.970931	0.004222	0.712384
-21.733848	-1.625687	0.975936	0.004173	0.712388
-21.960542	-1.589086	0.980941	0.004215	0.712381
-21.755100	-1.621530	0.985946	0.004177	0.712389
-21.985396	-1.584288	0.990950	0.004220	0.712382
-21.770126	-1.622127	0.995955	0.004179	0.712383
-22.178802	-1.607715	1.000960	0.004255	0.712267
-23.223467	-1.513103	1.005965	0.004450	0.712085
-22.320310	-1.669247	1.010970	0.004281	0.712095
-22.705817	-1.603210	1.015974	0.004353	0.712090
-23.045241	-1.543739	1.020979	0.004416	0.712088
-22.222410	-1.688977	1.025984	0.004263	0.712091
-22.656393	-1.615751	1.030989	0.004343	0.712083
-22.741629	-1.603727	1.035994	0.004359	0.712077
-23.221175	-1.679159	1.040998	0.004448	0.711757
-23.411241	-1.645205	1.046003	0.004483	0.711757
-23.523280	-1.622374	1.051008	0.004504	0.711763
-23.616074	-1.610450	1.056013	0.004521	0.711755
-23.390122	-1.646437	1.061018	0.004479	0.711763
-23.609303	-1.610074	1.066022	0.004520	0.711758
-23.789895	-1.578317	1.071027	0.004553	0.711758
-23.964383	-1.688622	1.076032	0.004585	0.711476
-24.555857	-1.598634	1.081037	0.004695	0.711446
-24.739272	-1.561129	1.086042	0.004729	0.711456
-24.476356	-1.610553	1.091046	0.004680	0.711451
-24.722936	-1.566215	1.096051	0.004726	0.711452
-24.506063	-1.601643	1.101056	0.004686	0.711459
-24.641284	-1.583722	1.106061	0.004711	0.711446
-24.560037	-1.661925	1.111066	0.004695	0.711320
-25.692559	-1.554139	1.116070	0.004906	0.711132
-25.587024	-1.572585	1.121075	0.004886	0.711133
-25.570010	-1.571971	1.126080	0.004883	0.711141
-25.298692	-1.625787	1.131085	0.004832	0.711130
-25.188293	-1.641619	1.136090	0.004811	0.711138
-25.291123	-1.625438	1.141094	0.004830	0.711134
-25.304066	-1.656913	1.146099	0.004833	0.711067
-25.943590	-1.641123	1.151104	0.004952	0.710871
-26.176141	-1.604248	1.156109	0.004995	0.710863
-26.016261	-1.629056	1.161114	0.004965	0.710870
-25.857769	-1.661318	1.166118	0.004935	0.710863
-26.303239	-1.579972	1.171123	0.005018	0.710867
-26.144698	-1.608725	1.176128	0.004988	0.710866
-26.151995	-1.718819	1.181133	0.004990	0.710644
-27.376598	-1.557596	1.186138	0.005217	0.710530
-27.310884	-1.573245	1.191142	0.005205	0.710523
-27.198959	-1.592831	1.196147	0.005184	0.710524
-27.328169	-1.566710	1.201152	0.005208	0.710530
-27.451985	-1.548936	1.206157	0.005231	0.710522
-27.073282	-1.611726	1.211162	0.005160	0.710532
-27.160615	-1.626515	1.216166	0.005176	0.710471
-28.003210	-1.606552	1.221171	0.005333	0.710212
-27.882532	-1.625902	1.226176	0.005310	0.710216
-28.356151	-1.546567	1.231181	0.005398	0.710206
-28.087448	-1.589758	1.236186	0.005348	0.710216
-28.127363	-1.585527	1.241190	0.005355	0.710211
-28.158403	-1.579324	1.246195	0.005361	0.710212
-27.729291	-1.657116	1.251200	0.005281	0.710210
-28.682708	-1.651432	1.256205	0.005458	0.709882
-28.820007	-1.622310	1.261210	0.005484	0.709891
-29.040603	-1.585097	1.266214	0.005525	0.709888
-29.224826	-1.553312	1.271219	0.005559	0.709886
-29.065460	-1.579285	1.276224	0.005529	0.709891
-29.094800	-1.576000	1.281229	0.005534	0.709887
-29.014946	-1.586905	1.286234	0.005519	0.709894
-29.567117	-1.562853	1.291238	0.005622	0.709746
-30.195618	-1.528418	1.296243	0.005739	0.709591
-29.341280	-1.678405	1.301248	0.005580	0.709596
-30.052833	-1.555839	1.306253	0.005712	0.709588
-29.920933	-1.574266	1.311258	0.005687	0.709598
-29.606501	-1.633885	1.316262	0.005629	0.709591
-30.064578	-1.551811	1.321267	0.005714	0.709592
-29.970519	-1.632672	1.326272	0.005696	0.709465
-30.674989	-1.612084	1.331277	0.005827	0.709255
-30.551401	-1.629929	1.336282	0.005804	0.709263
-30.852133	-1.579912	1.341286	0.005860	0.709257
-30.868675	-1.574265	1.346291	0.005863	0.709262
-30.524852	-1.633896	1.351296	0.005798	0.709266
-31.084280	-1.538905	1.356301	0.005902	0.709257
-30.694759	-1.655157	1.361306	0.005830	0.709163
-31.441609	-1.629735	1.366310	0.005969	0.708948
-31.746367	-1.575723	1.371315	0.006025	0.708948
-31.829083	-1.555750	1.376320	0.006041	0.708959
-31.720704	-1.580126	1.381325	0.006020	0.708949
-31.441847	-1.625568	1.386330	0.005968	0.708958
-31.646176	-1.591600	1.391334	0.006006	0.708953
-31.824182	-1.596666	1.396339	0.006039	0.708880
-32.205332	-1.647285	1.401344	0.006110	0.708642
-32.454637	-1.607364	1.406349	0.006156	0.708634
-32.622731	-1.575059	1.411354	0.006187	0.708639
-32.439838	-1.609441	1.416358	0.006153	0.708635
-32.525057	-1.594946	1.421363	0.006169	0.708634
-32.747564	-1.551501	1.426368	0.006210	0.708642
-32.785864	-1.559474	1.431373	0.006217	0.708613
-32.981786	-1.654743	1.436378	0.006253	0.708352
-33.310606	-1.599284	1.441382	0.006314	0.708346
-33.709011	-1.528891	1.446387	0.006388	0.708345
-33.050947	-1.643562	1.451392	0.006266	0.708351
-33.339168	-1.597754	1.456397	0.006319	0.708340
-33.518534	-1.562428	1.461402	0.006352	0.708347
-33.172909	-1.659854	1.466406	0.006288	0.708276
-34.304480	-1.591717	1.471411	0.006499	0.708008
-34.283582	-1.592087	1.476416	0.006494	0.708015
-34.479029	-1.563122	1.481421	0.006531	0.708004
-34.183418	-1.611482	1.486426	0.006476	0.708013
-34.234096	-1.605595	1.491430	0.006485	0.708007
-34.339816	-1.586978	1.496435	0.006504	0.708007
-33.939299	-1.690980	1.501440	0.006430	0.707941
-35.196137	-1.591068	1.506445	0.006663	0.707693
-35.137143	-1.597256	1.511450	0.006652	0.707702
-35.251357	-1.578915	1.516454	0.006673	0.707698
-35.293533	-1.575281	1.521459	0.006681	0.707691
-35.271736	-1.574334	1.526464	0.006677	0.707701
-35.304427	-1.572741	1.531469	0.006683	0.707692
-35.099525	-1.605053	1.536474	0.006645	0.707701
-35.842680	-1.636909	1.541478	0.006783	0.707372
-36.360882	-1.545741	1.546483	0.006879	0.707370
-36.044758	-1.598620	1.551488	0.006820	0.707377
-36.116677	-1.589916	1.556493	0.006833	0.707369
-36.356276	-1.542495	1.561498	0.006878	0.707379
-36.035491	-1.605072	1.566502	0.006818	0.707368
-35.988673	-1.613138	1.571507	0.006809	0.707369
-36.174033	-1.679449	1.576512	0.006843	0.707170
-37.268203	-1.532618	1.581517	0.007047	0.707073
-36.807100	-1.610292	1.586522	0.006961	0.707083
-36.983558	-1.580425	1.591526	0.006994	0.707080
-37.521076	-1.486122	1.596531	0.007094	0.707077
-36.846315	-1.602892	1.601536	0.006968	0.707085
-36.935972	-1.591996	1.606541	0.006984	0.707075
-37.134831	-1.651776	1.611546	0.007021	0.706884
-37.722550	-1.613849	1.616550	0.007130	0.706750
-37.616756	-1.633943	1.621555	0.007111	0.706748
-37.876732	-1.584525	1.626560	0.007159	0.706754
-38.128784	-1.543979	1.631565	0.007206	0.706746
-37.734298	-1.610832	1.636570	0.007132	0.706753
-37.808320	-1.600079	1.641574	0.007146	0.706748
-38.381353	-1.599057	1.646579	0.007252	0.706545
-38.593641	-1.611432	1.651584	0.007292	0.706445
-38.539850	-1.626101	1.656589	0.007281	0.706435
-38.549944	-1.622275	1.661594	0.007283	0.706439
-38.849349	-1.570490	1.666598	0.007339	0.706436
-38.758966	-1.588109	1.671603	0.007322	0.706434
-38.529469	-1.624506	1.676608	0.007279	0.706443
-39.071189	-1.646724	1.681613	0.007380	0.706205
-39.875247	-1.541510	1.686618	0.007529	0.706128
-39.668576	-1.579664	1.691622	0.007490	0.706126
-39.900386	-1.541246	1.696627	0.007533	0.706120
-39.561795	-1.597365	1.701632	0.007470	0.706129
-39.693134	-1.579769	1.706637	0.007495	0.706118
-39.878253	-1.543773	1.711642	0.007529	0.706124
-39.622540	-1.625336	1.716646	0.007481	0.706052
-40.392896	-1.586895	1.721651	0.007624	0.705853
-39.978669	-1.655918	1.726656	0.007547	0.705863
-40.635002	-1.544770	1.731661	0.007669	0.705852
-40.141905	-1.629405	1.736666	0.007577	0.705859
-39.976182	-1.658242	1.741670	0.007546	0.705861
-40.817404	-1.511341	1.746675	0.007703	0.705855
-40.709583	-1.659832	1.751680	0.007683	0.705595
-41.451041	-1.565505	1.756685	0.007820	0.705519
-41.505535	-1.553805	1.761690	0.007830	0.705523
-41.184792	-1.613032	1.766694	0.007771	0.705520
-41.311034	-1.591878	1.771699	0.007794	0.705517
-41.314715	-1.586134	1.776704	0.007794	0.705528
-41.687336	-1.524006	1.781709	0.007864	0.705519
-41.644463	-1.632162	1.786714	0.007855	0.705317
-42.260242	-1.575303	1.791718	0.007970	0.705211
-42.522697	-1.530214	1.796723	0.008019	0.705208
-41.993504	-1.623036	1.801728	0.007920	0.705211
-42.183600	-1.594684	1.806733	0.007955	0.705201
-42.098246	-1.604970	1.811738	0.007939	0.705211
-42.137144	-1.599424	1.816742	0.007946	0.705208
-42.613959	-1.634305	1.821747	0.008035	0.704967
-43.231693	-1.563234	1.826752	0.008150	0.704889
-43.232439	-1.567163	1.831757	0.008150	0.704881
-42.796575	-1.641954	1.836762	0.008068	0.704887
-42.876809	-1.628419	1.841766	0.008083	0.704886
-43.190693	-1.575438	1.846771	0.008141	0.704880
-42.966077	-1.611328	1.851776	0.008100	0.704889
-43.147607	-1.701854	1.856781	0.008133	0.704642
-44.071174	-1.564192	1.861786	0.008305	0.704587
-44.262334	-1.530416	1.866790	0.008340	0.704587
-43.937546	-1.590365	1.871795	0.008280	0.704583
-43.776228	-1.614509	1.876800	0.008250	0.704593
-44.276703	-1.529654	1.881805	0.008343	0.704584
-44.191631	-1.541716	1.886810	0.008327	0.704591
-44.093094	-1.666899	1.891814	0.008308	0.704374
-45.254887	-1.519544	1.896819	0.008524	0.704254
-44.876428	-1.582442	1.901824	0.008454	0.704264
-44.958852	-1.573974	1.906829	0.008469	0.704251
-45.094787	-1.547216	1.911834	0.008494	0.704257
-44.849808	-1.591698	1.916838	0.008448	0.704255
-44.904694	-1.583184	1.921843	0.008458	0.704253
-44.807516	-1.673664	1.926848	0.008440	0.704106
-46.087123	-1.526328	1.931853	0.008678	0.703943
-45.739367	-1.583330	1.936858	0.008613	0.703954
-45.542449	-1.621024	1.941862	0.008576	0.703949
-45.953447	-1.549483	1.946867	0.008653	0.703946
-45.885210	-1.557231	1.951872	0.008640	0.703955
-45.689490	-1.598117	1.956877	0.008603	0.703943
-45.537586	-1.686676	1.961882	0.008575	0.703819
-46.642686	-1.581553	1.966886	0.008781	0.703634
-46.666989	-1.580270	1.971891	0.008785	0.703628
-46.273622	-1.645640	1.976896	0.008712	0.703638
-46.690557	-1.577911	1.981901	0.008789	0.703625
-46.702491	-1.572954	1.986906	0.008791	0.703631
-46.547713	-1.601471	1.991910	0.008762	0.703630
-46.926295	-1.626162	1.996915	0.008832	0.703444
-47.326598	-1.609566	2.001920	0.008907	0.703334

-47.255072	-1.621880	2.011917	0.008893	0.703335
-47.407894	-1.593148	2.021914	0.008921	0.703339
-47.703014	-1.542993	2.031910	0.008976	0.703334
-47.374229	-1.602956	2.041907	0.008914	0.703332
-47.532859	-1.572917	2.051904	0.008944	0.703336
-47.472703	-1.582158	2.061901	0.008932	0.703340
-47.383200	-1.598916	2.071898	0.008915	0.703339
-47.456850	-1.587281	2.081894	0.008929	0.703337
-47.265013	-1.621665	2.091891	0.008893	0.703337
-47.593133	-1.562723	2.101888	0.008953	0.703338
-47.429648	-1.592168	2.111885	0.008923	0.703338
-47.604564	-1.562323	2.121882	0.008955	0.703336
-47.576980	-1.567189	2.131878	0.008949	0.703337
-46.755905	-1.574839	2.141875	0.008796	0.703617
-46.627858	-1.589368	2.151872	0.008772	0.703635
-46.319086	-1.645374	2.161869	0.008714	0.703634
-46.621979	-1.591861	2.171866	0.008770	0.703633
-46.786980	-1.555303	2.181862	0.008801	0.703648
-45.916241	-1.563953	2.191859	0.008638	0.703944
-45.801583	-1.582870	2.201856	0.008617	0.703948
-45.630108	-1.613002	2.211853	0.008584	0.703950
-45.827368	-1.569838	2.221850	0.008621	0.703966
-44.944617	-1.584238	2.231846	0.008456	0.704255
-44.646045	-1.639664	2.241843	0.008400	0.704251
-44.814957	-1.608916	2.251840	0.008431	0.704253
-44.706466	-1.625337	2.261837	0.008411	0.704260
-44.128415	-1.567587	2.271834	0.008303	0.704585
-43.834408	-1.621075	2.281830	0.008248	0.704583
-43.946009	-1.601824	2.291827	0.008268	0.704582
-44.140472	-1.523935	2.301824	0.008304	0.704670
-43.037815	-1.614593	2.311821	0.008099	0.704884
-43.276867	-1.572156	2.321818	0.008143	0.704884
-43.124168	-1.601809	2.331814	0.008114	0.704880
-42.825543	-1.519556	2.341811	0.008058	0.705153
-42.494143	-1.552964	2.351808	0.007996	0.705206
-42.326455	-1.582222	2.361805	0.007965	0.705207
-42.139333	-1.531476	2.371802	0.007929	0.705377
-41.413201	-1.592447	2.381798	0.007794	0.705516
-41.496464	-1.577279	2.391795	0.007809	0.705517
-41.283516	-1.614799	2.401792	0.007769	0.705518
-40.828269	-1.536829	2.411789	0.007684	0.705839
-40.688374	-1.553399	2.421786	0.007658	0.705857
-40.330605	-1.618677	2.431782	0.007591	0.705854
-40.608032	-1.512862	2.441779	0.007642	0.705968
-39.778925	-1.584662	2.451776	0.007488	0.706122
-39.732651	-1.592313	2.461773	0.007479	0.706123
-39.958657	-1.530669	2.471770	0.007520	0.706167
-38.927757	-1.581019	2.481766	0.007328	0.706436
-39.181797	-1.534826	2.491763	0.007375	0.706438
-39.011184	-1.565729	2.501760	0.007343	0.706438
-38.529004	-1.521284	2.511757	0.007253	0.706700
-38.245315	-1.549584	2.521754	0.007200	0.706746
-38.234890	-1.552361	2.531750	0.007198	0.706744
-37.905404	-1.515781	2.541747	0.007136	0.706936
-37.143426	-1.583359	2.551744	0.006994	0.707074
-37.312653	-1.552790	2.561741	0.007025	0.707075
-37.314348	-1.527247	2.571738	0.007025	0.707127
-36.486346	-1.555016	2.581734	0.006870	0.707368
-36.627731	-1.530072	2.591731	0.006896	0.707368
-36.495422	-1.553835	2.601728	0.006871	0.707368
-36.070024	-1.491564	2.611725	0.006792	0.707646
-35.572100	-1.556105	2.621722	0.006699	0.707695
-35.720522	-1.530102	2.631718	0.006726	0.707695
-35.304699	-1.522920	2.641715	0.006648	0.707858
-34.635690	-1.569809	2.651712	0.006524	0.708004
-34.664735	-1.563175	2.661709	0.006529	0.708007
-34.676972	-1.561991	2.671706	0.006531	0.708006
-33.995784	-1.519166	2.681702	0.006404	0.708336
-33.842041	-1.543900	2.691699	0.006375	0.708342
-33.695458	-1.568723	2.701696	0.006347	0.708345
-33.580215	-1.522553	2.711693	0.006325	0.708479
-32.829646	-1.578366	2.721690	0.006185	0.708636
-33.139248	-1.523833	2.731686	0.006242	0.708635
-33.073511	-1.529252	2.741683	0.006230	0.708648
-32.105885	-1.551798	2.751680	0.006049	0.708949
-32.068946	-1.556765	2.761677	0.006042	0.708953
-31.967158	-1.575905	2.771674	0.006023	0.708952
-31.850737	-1.524300	2.781670	0.006001	0.709097
-31.062699	-1.583903	2.791667	0.005854	0.709260
-31.246303	-1.549876	2.801664	0.005888	0.709263
-31.258655	-1.548790	2.811661	0.005890	0.709261
-30.474555	-1.526803	2.821658	0.005744	0.709585
-30.287620	-1.557679	2.831654	0.005708	0.709591
-30.310277	-1.553820	2.841651	0.005712	0.709591
-30.134145	-1.516578	2.851648	0.005679	0.709729
-29.334869	-1.578375	2.861645	0.005530	0.709891
-29.303326	-1.584527	2.871642	0.005524	0.709890
-29.527691	-1.544799	2.881638	0.005565	0.709890
-28.710078	-1.540437	2.891635	0.005413	0.710191
-28.351407	-1.594524	2.901632	0.005346	0.710211
-28.436447	-1.578492	2.911629	0.005361	0.710213
-28.389479	-1.544451	2.921626	0.005352	0.710299
-27.730497	-1.548309	2.931622	0.005229	0.710526
-27.657103	-1.562428	2.941619	0.005215	0.710525
-27.629728	-1.565685	2.951616	0.005210	0.710529
-27.009786	-1.539296	2.961613	0.005094	0.710803
-26.771292	-1.549565	2.971610	0.005049	0.710867
-26.997714	-1.510569	2.981606	0.005091	0.710865
-26.551110	-1.546841	2.991603	0.005008	0.710952
-25.944181	-1.564022	3.001600	0.004894	0.711135
-25.920082	-1.567281	3.011597	0.004890	0.711137
-25.893297	-1.571411	3.021594	0.004884	0.711139
-25.400035	-1.516404	3.031590	0.004792	0.711425
-25.037012	-1.567755	3.041587	0.004724	0.711452
-25.042731	-1.566406	3.051584	0.004725	0.711453
-24.737730	-1.551972	3.061581	0.004668	0.711591
-23.997368	-1.596798	3.071578	0.004530	0.711765
-24.207234	-1.559737	3.081574	0.004569	0.711765
-23.958846	-1.606096	3.091571	0.004522	0.711762
-23.377345	-1.579500	3.101568	0.004413	0.712022
-23.360208	-1.547283	3.111565	0.004410	0.712093
-23.204883	-1.575020	3.121562	0.004381	0.712093
-23.309842	-1.518338	3.131558	0.004400	0.712169
-22.344441	-1.583645	3.141555	0.004220	0.712383
-22.407233	-1.569182	3.151552	0.004231	0.712390
-22.311736	-1.587161	3.161549	0.004213	0.712388
-21.824276	-1.540897	3.171546	0.004122	0.712654
-21.690323	-1.537979	3.181542	0.004097	0.712708
-21.145502	-1.636528	3.191539	0.003995	0.712706
-21.443293	-1.540978	3.201536	0.004050	0.712791
-20.336845	-1.621650	3.211533	0.003844	0.713023
-20.423700	-1.606628	3.221530	0.003860	0.713023
-20.717947	-1.556067	3.231526	0.003914	0.713020
-19.985182	-1.581234	3.241523	0.003777	0.713230
-19.670174	-1.573464	3.251520	0.003718	0.713358
-19.346103	-1.631028	3.261517	0.003658	0.713359
-19.677327	-1.571249	3.271514	0.003719	0.713361
-18.977887	-1.567666	3.281510	0.003589	0.713616
-18.738455	-1.594663	3.291507	0.003544	0.713648
-18.655237	-1.608803	3.301504	0.003528	0.713650
-18.344220	-1.629843	3.311501	0.003470	0.713719
-17.792937	-1.602977	3.321498	0.003367	0.713968
-17.502523	-1.655643	3.331494	0.003312	0.713967
-17.706693	-1.619603	3.341491	0.003350	0.713967
-17.644795	-1.560176	3.351488	0.003338	0.714108
-16.422894	-1.690720	3.361485	0.003111	0.714281
-16.889770	-1.608743	3.371482	0.003197	0.714280
-16.764083	-1.633083	3.381478	0.003173	0.714276
-16.028516	-1.631149	3.391475	0.003036	0.714541
-15.989918	-1.603725	3.401472	0.003029	0.714610
-15.650363	-1.663294	3.411469	0.002965	0.714612
-15.901392	-1.615916	3.421466	0.003012	0.714618
-15.095354	-1.614142	3.431462	0.002861	0.714907
-14.964417	-1.638985	3.441459	0.002836	0.714905
-14.801918	-1.667719	3.451456	0.002806	0.714906
-14.689402	-1.631665	3.461453	0.002785	0.715018
-14.071897	-1.635299	3.471450	0.002669	0.715229
-13.986848	-1.651022	3.481446	0.002653	0.715229
-14.069253	-1.636992	3.491443	0.002668	0.715228
-13.370239	-1.659762	3.501440	0.002538	0.715430
-13.053691	-1.659538	3.511437	0.002479	0.715543
-13.184908	-1.636261	3.521434	0.002503	0.715544
-12.983236	-1.673036	3.531430	0.002465	0.715542
-12.358268	-1.618016	3.541427	0.002348	0.715873
-12.041794	-1.671140	3.551424	0.002289	0.715880
-12.195976	-1.642669	3.561421	0.002317	0.715882
-12.075116	-1.621784	3.571418	0.002294	0.715967
-11.002205	-1.731870	3.581414	0.002094	0.716128
-11.336263	-1.673842	3.591411	0.002156	0.716126
-11.237063	-1.690271	3.601408	0.002137	0.716129
-10.806197	-1.663552	3.611405	0.002057	0.716334
-10.479932	-1.664980	3.621402	0.001996	0.716447
-10.545292	-1.654147	3.631398	0.002008	0.716446
-10.757315	-1.576140	3.641395	0.002047	0.716527
-9.461957	-1.692413	3.651392	0.001805	0.716754
-9.542685	-1.676908	3.661389	0.001820	0.716757
-9.532124	-1.678572	3.671386	0.001818	0.716758
-8.815118	-1.680762	3.681382	0.001684	0.717007
-8.671959	-1.669031	3.691379	0.001657	0.717081
-8.431410	-1.710752	3.701376	0.001612	0.717084
-8.564404	-1.685818	3.711373	0.001636	0.717087
-7.884605	-1.660648	3.721370	0.001510	0.717377
-7.881674	-1.660518	3.731366	0.001509	0.717378
-7.806730	-1.674716	3.741363	0.001494	0.717377
-7.278472	-1.684835	3.751360	0.001396	0.717544
-6.795295	-1.689513	3.761357	0.001305	0.717705
-6.660898	-1.714419	3.771354	0.001280	0.717704
-6.711288	-1.706333	3.781350	0.001289	0.717703
-6.177638	-1.685887	3.791347	0.001190	0.717932
-5.819600	-1.707036	3.801344	0.001123	0.718016
-5.860483	-1.700208	3.811341	0.001130	0.718016
-5.598112	-1.746286	3.821338	0.001081	0.718018
-5.214867	-1.644541	3.831334	0.001009	0.718354
-5.011653	-1.680714	3.841331	0.000971	0.718355
-4.706798	-1.736138	3.851328	0.000914	0.718353
-4.710065	-1.684239	3.861325	0.000914	0.718455
-3.713745	-1.766495	3.871322	0.000728	0.718644
-4.151471	-1.691087	3.881318	0.000809	0.718639
-4.012805	-1.715091	3.891315	0.000783	0.718641
-3.483219	-1.696805	3.901312	0.000684	0.718864
-3.190604	-1.699862	3.911309	0.000630	0.718961
-3.174331	-1.704284	3.921306	0.000626	0.718959
-3.046716	-1.706867	3.931302	0.000602	0.718999
-2.463716	-1.675207	3.941299	0.000493	0.719267
-2.381075	-1.691568	3.951296	0.000478	0.719265
-2.413598	-1.685200	3.961293	0.000483	0.719266
-2.258203	-1.580939	3.971290	0.000454	0.719527
-1.842602	-1.619687	3.981286	0.000376	0.719597
-1.839878	-1.621301	3.991283	0.000376	0.719595
-1.751788	-1.512368	4.001280	0.000359	0.719842
-1.148163	-1.591367	4.011277	0.000246	0.719898
-1.256030	-1.572453	4.021274	0.000266	0.719898
-1.004865	-1.455999	4.031270	0.000219	0.720216
-1.057142	-1.444604	4.041267	0.000228	0.720221
-1.209087	-1.336201	4.051264	0.000256	0.720382
-1.232443	-1.252348	4.061261	0.000260	0.720539
-0.983339	-1.215844	4.071258	0.000213	0.720699
-0.542650	-1.204978	4.081254	0.000131	0.720875
-0.642200	-1.136819	4.091251	0.000149	0.720975
-0.542923	-1.083081	4.101248	0.000130	0.721116
-0.568436	-0.981869	4.111245	0.000135	0.721307
-0.705725	-0.889351	4.121242	0.000160	0.721441
-0.591971	-0.765972	4.131238	0.000138	0.721724
-0.635082	-0.681633	4.141235	0.000146	0.721876
-0.203915	-0.659130	4.151232	0.000065	0.722071
-0.250317	-0.510728	4.161229	0.000074	0.722347
-0.383810	-0.390323	4.171226	0.000098	0.722537
-0.420777	-0.270194	4.181222	0.000105	0.722761
-0.357387	-0.159653	4.191219	0.000092	0.723000
-0.336260	0.003768	4.201216	0.000088	0.723329
-0.303513	0.120300	4.211213	0.000082	0.723569
0.000000	0.213338	4.221210	0.000025	0.723858

0.072953	0.851159	4.226214	0.000011	0.725132
0.087801	2.107710	4.231219	0.000007	0.727591
0.383341	3.936988	4.236224	-0.000050	0.731251
0.437979	6.342088	4.241229	-0.000061	0.735920
0.676178	9.230327	4.246234	-0.000108	0.741546
0.933245	12.600718	4.251238	-0.000158	0.748051
1.279642	16.392031	4.256243	-0.000225	0.755321
1.692340	20.590613	4.261248	-0.000305	0.763300
2.009504	25.202267	4.266253	-0.000367	0.771925
2.532402	30.143842	4.271258	-0.000468	0.781120
2.805747	35.483941	4.276262	-0.000522	0.790843
3.223480	41.099630	4.281267	-0.000604	0.800981
3.772021	47.011888	4.286272	-0.000710	0.811551
4.301353	53.198968	4.291277	-0.000813	0.822453
4.681844	59.696148	4.296282	-0.000888	0.833695
5.201493	66.378953	4.301286	-0.000989	0.845140
5.545016	73.314971	4.306291	-0.001058	0.856800
6.012509	80.442513	4.311296	-0.001150	0.868651
6.484576	87.743591	4.316301	-0.001243	0.880623
7.065813	95.206043	4.321306	-0.001356	0.892722
7.624162	102.834377	4.326310	-0.001465	0.904911
8.247881	110.595026	4.331315	-0.001586	0.917161
9.140867	118.443488	4.336320	-0.001758	0.929455
9.649648	126.460259	4.341325	-0.001858	0.941740
10.031898	134.613300	4.346330	-0.001935	0.954036
10.940258	142.761617	4.351334	-0.002109	0.966303
11.857011	150.991119	4.356339	-0.002285	0.978535
12.649986	159.336812	4.361344	-0.002439	0.990752
13.262500	167.738888	4.366349	-0.002558	1.002854
14.167389	176.147031	4.371354	-0.002733	1.014892
15.221035	184.574171	4.376358	-0.002934	1.026849
15.532581	193.172281	4.381363	-0.002998	1.038726
16.342252	201.714050	4.386368	-0.003155	1.050509
16.896804	210.315991	4.391373	-0.003264	1.062182
17.818284	218.898903	4.396378	-0.003441	1.073787
18.506149	227.513711	4.401382	-0.003575	1.085256
18.971136	236.174387	4.406387	-0.003667	1.096614
19.544625	244.824099	4.411392	-0.003780	1.107865
20.137422	253.469355	4.416397	-0.003896	1.119002
21.035626	262.063205	4.421402	-0.004069	1.130030
21.835699	270.686366	4.426406	-0.004224	1.140966
22.460108	279.351837	4.431411	-0.004346	1.151813
23.073874	287.991469	4.436416	-0.004466	1.162524
23.669169	296.615282	4.441421	-0.004582	1.173115
24.127306	305.247378	4.446426	-0.004674	1.183592
24.650088	313.870108	4.451430	-0.004777	1.193980
25.322216	322.422021	4.456435	-0.004908	1.204223
26.330451	330.941585	4.461440	-0.005101	1.214410
26.983933	339.497837	4.466445	-0.005228	1.224483
27.652969	348.076021	4.471450	-0.005359	1.234502
28.082628	356.642983	4.476454	-0.005444	1.244382
28.310171	365.228230	4.481459	-0.005493	1.254165
29.308507	373.677411	4.486464	-0.005684	1.263866
29.768029	382.211457	4.491469	-0.005775	1.273486
29.967754	390.755077	4.496474	-0.005818	1.282996
30.705356	399.212287	4.501478	-0.005961	1.292440
31.300177	407.667416	4.506483	-0.006078	1.301787
31.993286	416.181888	4.511488	-0.006212	1.311149
32.309213	424.701611	4.516493	-0.006277	1.320382
32.826437	433.109373	4.521498	-0.006379	1.329467
33.497478	441.500264	4.526502	-0.006510	1.338500
33.980125	449.893510	4.531507	-0.006605	1.347441
34.596634	458.290791	4.536512	-0.006725	1.356351
34.907593	466.695419	4.541517	-0.006789	1.365157
35.359141	475.088374	4.546522	-0.006879	1.373918
36.155868	483.415560	4.551526	-0.007033	1.382616
36.683897	491.796634	4.556531	-0.007137	1.391268
36.899110	500.208155	4.561536	-0.007182	1.399844
37.139133	508.569985	4.566541	-0.007233	1.408323
37.677340	516.896646	4.571546	-0.007338	1.416765
38.164658	525.213942	4.576550	-0.007435	1.425138
38.681294	533.528403	4.581555	-0.007536	1.433465
39.394144	541.800588	4.586560	-0.007675	1.441734
40.087752	550.074495	4.591565	-0.007809	1.449953
40.298847	558.431860	4.596570	-0.007854	1.458131
40.895052	566.716246	4.601574	-0.007971	1.466253
41.076828	575.104701	4.606579	-0.008010	1.474364
41.543569	583.381118	4.611584	-0.008103	1.482369
41.777577	591.682747	4.616589	-0.008152	1.490319
42.399726	599.925710	4.621594	-0.008273	1.498230
42.827266	608.195095	4.626598	-0.008358	1.506095
43.148581	616.483102	4.631603	-0.008424	1.513920
43.851148	624.690864	4.636608	-0.008560	1.521688
44.388509	632.923546	4.641613	-0.008666	1.529414
44.829440	641.189018	4.646618	-0.008753	1.537117
45.230928	649.447469	4.651622	-0.008834	1.544769
45.677718	657.703650	4.656627	-0.008922	1.552388
46.162545	665.937085	4.661632	-0.009018	1.559954
46.487183	674.173980	4.666637	-0.009084	1.567463
46.938259	682.414451	4.671642	-0.009174	1.574958
47.339991	690.645353	4.676646	-0.009254	1.582402
47.459308	698.908104	4.681651	-0.009282	1.589798
47.874659	707.145740	4.686656	-0.009365	1.597181
48.540586	715.299557	4.691661	-0.009494	1.604490
48.928033	723.526807	4.696666	-0.009572	1.611792
49.445659	731.736211	4.701670	-0.009674	1.619063
50.094942	739.900795	4.706675	-0.009800	1.626280
50.670124	748.160359	4.711680	-0.009913	1.633538
50.872479	756.367135	4.716685	-0.009956	1.640666
51.261046	764.556223	4.721690	-0.010034	1.647774
51.921642	772.728352	4.726694	-0.010162	1.654873
52.245339	780.922691	4.731699	-0.010228	1.661916
52.437192	789.152156	4.736704	-0.010269	1.668940
52.767976	797.350180	4.741709	-0.010336	1.675927
52.978502	805.545666	4.746714	-0.010381	1.682867
53.491331	813.704328	4.751718	-0.010482	1.689787
53.843395	821.884649	4.756723	-0.010553	1.696676
54.369243	830.050361	4.761728	-0.010656	1.703548
54.476913	838.272376	4.766733	-0.010682	1.710383
55.013232	846.423052	4.771738	-0.010787	1.717189
55.738927	854.542107	4.776742	-0.010928	1.723966
55.872401	862.738618	4.781747	-0.010958	1.730703
56.231085	870.928480	4.786752	-0.011030	1.737437
56.853549	879.044800	4.791757	-0.011152	1.744119
57.197169	887.221669	4.796762	-0.011221	1.750790
57.280981	895.441054	4.801766	-0.011242	1.757436
57.596982	903.576499	4.806771	-0.011307	1.764019
58.366727	911.683489	4.811776	-0.011455	1.770611
58.870295	919.833915	4.816781	-0.011555	1.777180
59.220698	927.992823	4.821786	-0.011625	1.783712
59.619273	936.181446	4.826790	-0.011705	1.790250
59.882070	944.379089	4.831795	-0.011760	1.796755
60.400816	952.498911	4.836800	-0.011862	1.803206
60.547812	960.662338	4.841805	-0.011894	1.809623
60.880039	968.817698	4.846810	-0.011962	1.816033
61.321059	976.939833	4.851814	-0.012049	1.822408
61.657215	985.078381	4.856819	-0.012117	1.828761
62.199558	993.213649	4.861824	-0.012224	1.835113
62.847603	1001.298469	4.866829	-0.012350	1.841417
62.996598	1009.469059	4.871834	-0.012383	1.847707
63.390238	1017.630776	4.876838	-0.012462	1.853997
63.689718	1025.752158	4.881843	-0.012523	1.860223
63.934233	1033.903695	4.886848	-0.012574	1.866446
64.243536	1042.070112	4.891853	-0.012637	1.872666
64.549582	1050.200065	4.896858	-0.012700	1.878838
64.880241	1058.307377	4.901862	-0.012767	1.884976
64.898131	1066.467316	4.906867	-0.012775	1.891097
65.424799	1074.580440	4.911872	-0.012879	1.897221
65.799698	1082.680967	4.916877	-0.012954	1.903299
65.733672	1090.856644	4.921882	-0.012947	1.909363
66.356146	1098.945674	4.926886	-0.013069	1.915421
66.658733	1107.045660	4.931891	-0.013130	1.921433
67.082283	1115.164950	4.936896	-0.013215	1.927453
67.309743	1123.312707	4.941901	-0.013263	1.933453
67.499969	1131.441562	4.946906	-0.013303	1.939417
67.915350	1139.546128	4.951910	-0.013386	1.945370
68.167791	1147.693686	4.956915	-0.013439	1.951318
68.814635	1155.784991	4.961920	-0.013565	1.957249
69.202703	1163.854435	4.966925	-0.013642	1.963119
69.525254	1171.956006	4.971930	-0.013708	1.968987
69.938448	1180.075693	4.976934	-0.013790	1.974861
70.197475	1188.169526	4.981939	-0.013844	1.980682
70.488064	1196.286213	4.986944	-0.013903	1.986505
70.727230	1204.427819	4.991949	-0.013953	1.992324
71.116888	1212.514689	4.996954	-0.014031	1.998103
71.439533	1220.630614	5.001958	-0.014097	2.003878
71.627110	1228.732408	5.006963	-0.014137	2.009613
71.974873	1236.861157	5.011968	-0.014207	2.015366
72.299790	1244.953075	5.016973	-0.014273	2.021076
72.576704	1253.056690	5.021978	-0.014330	2.026772
73.226466	1261.157997	5.026982	-0.014457	2.032489
73.531793	1269.259395	5.031987	-0.014519	2.038154
73.630095	1277.377285	5.036992	-0.014543	2.043794
73.623455	1285.511401	5.041997	-0.014547	2.049419
73.884084	1293.613752	5.047002	-0.014601	2.055034
74.376638	1301.684999	5.052006	-0.014698	2.060635
74.642494	1309.768457	5.057011	-0.014753	2.066207
75.051750	1317.869712	5.062016	-0.014835	2.071790
75.305474	1325.972533	5.067021	-0.014887	2.077344
75.715661	1334.035885	5.072026	-0.014969	2.082871
75.952581	1342.149180	5.077030	-0.015019	2.088401
76.060309	1350.268759	5.082035	-0.015044	2.093907
76.354664	1358.364925	5.087040	-0.015104	2.099401
76.652936	1366.425335	5.092045	-0.015165	2.104857
77.194738	1374.520105	5.097050	-0.015272	2.110346
77.438185	1382.686936	5.102054	-0.015322	2.115840
77.918572	1390.702991	5.107059	-0.015417	2.121241
78.133951	1398.801480	5.112064	-0.015463	2.126658
78.235891	1406.924179	5.117069	-0.015487	2.132067
78.537442	1414.996260	5.122074	-0.015549	2.137447
78.860842	1423.068774	5.127078	-0.015614	2.142816
79.290900	1431.132539	5.132083	-0.015700	2.148176
79.845177	1439.216832	5.137088	-0.015809	2.153548
79.961232	1447.312895	5.142093	-0.015836	2.158872
80.075593	1455.397304	5.147098	-0.015862	2.164176
80.597056	1463.472614	5.152102	-0.015965	2.169499
80.614929	1471.605488	5.157107	-0.015974	2.174799
80.856978	1479.686951	5.162112	-0.016024	2.180074
81.161037	1487.748047	5.167117	-0.016086	2.185328
81.353666	1495.856651	5.172122	-0.016127	2.190591
81.550120	1503.980009	5.177126	-0.016169	2.195850
81.723168	1512.031861	5.182131	-0.016207	2.201049
82.340716	1520.042620	5.187136	-0.016327	2.206249
82.416222	1528.161542	5.192141	-0.016347	2.211458
82.759391	1536.233167	5.197146	-0.016416	2.216647
82.907301	1544.343314	5.202150	-0.016449	2.221832
83.062245	1552.406438	5.207155	-0.016484	2.226975
83.172973	1560.537121	5.212160	-0.016510	2.232146
83.475397	1568.590089	5.217165	-0.016571	2.237272
83.801346	1576.630517	5.222170	-0.016637	2.242381
84.271677	1584.688476	5.227174	-0.016730	2.247501
84.598158	1592.764077	5.232179	-0.016797	2.252608
84.843440	1600.870543	5.237184	-0.016848	2.257716
85.153357	1608.940396	5.242189	-0.016911	2.262795
85.359381	1617.016754	5.247194	-0.016955	2.267858
85.719650	1625.167184	5.252198	-0.017027	2.272969
85.930208	1633.216952	5.257203	-0.017072	2.277992
86.292501	1641.266714	5.262208	-0.017145	2.283018
86.645590	1649.307225	5.267213	-0.017216	2.288026
87.141792	1657.357789	5.272218	-0.017314	2.293041
87.482527	1665.427184	5.277222	-0.017382	2.298044
87.443025	1673.524456	5.282227	-0.017381	2.303021
87.976782	1681.558571	5.287232	-0.017485	2.307996
88.004293	1689.684583	5.292237	-0.017496	2.312975
88.116655	1697.750808	5.297242	-0.017522	2.317913
88.567128	1705.795584	5.302246	-0.017611	2.322856
88.769090	1713.857547	5.307251	-0.017654	2.327778
89.095568	1721.933667	5.312256	-0.017721	2.332709
89.228747	1730.010320	5.317261	-0.017751	2.337613
89.415286	1738.066296	5.322266	-0.017791	2.342500
89.770097	1746.135063	5.327270	-0.017863	2.347397
89.981344	1754.244262	5.332275	-0.017907	2.352297
90.128820	1762.328690	5.337280	-0.017940	2.357166
90.446028	1770.373675	5.342285	-0.018005	2.362015
90.503060	1778.428444	5.347290	-0.018021	2.366840
90.914838	1786.495909	5.352294	-0.018103	2.371690
91.158508	1794.551901	5.357299	-0.018154	2.376510
91.322169	1802.615192	5.362304	-0.018189	2.381319
91.810678	1810.659527	5.367309	-0.018286	2.386132
91.917149	1818.745183	5.372314	-0.018311	2.390929
92.207001	1826.836669	5.377318	-0.018370	2.395735
92.593257	1834.851218	5.382323	-0.018448	2.400494
93.176883	1842.875544	5.387328	-0.018562	2.405264
92.987058	1850.996489	5.392333	-0.018532	2.410021
93.216889	1859.089875	5.397338	-0.018580	2.414785
93.560532	1867.123436	5.402342	-0.018649	2.419513
93.716747	1875.186805	5.407347	-0.018684	2.424235
94.177208	1883.239171	5.412352	-0.018775	2.428965
94.520538	1891.365981	5.417357	-0.018844	2.433720
94.854282	1899.387213	5.422362	-0.018912	2.438403
95.275874	1907.425737	5.427366	-0.018996	2.443094
95.597414	1915.443986	5.432371	-0.019061	2.447757
95.928497	1923.525745	5.437376	-0.019128	2.452448
96.209283	1931.596985	5.442381	-0.019186	2.457120
96.349043	1939.641927	5.447386	-0.019217	2.461758
96.740545	1947.703262	5.452390	-0.019296	2.466415
97.037978	1955.764009	5.457395	-0.019356	2.471056
97.106445	1963.861748	5.462400	-0.019375	2.475692
97.634608	1971.877138	5.467405	-0.019478	2.480307
97.919905	1979.920704	5.472410	-0.019537	2.484911
98.073144	1988.008871	5.477414	-0.019571	2.489522
98.208026	1996.096628	5.482419	-0.019601	2.494123
98.520141	2004.139266	5.487424	-0.019665	2.498703
98.744139	2012.194431	5.492429	-0.019712	2.503275
99.117281	2020.230022	5.497434	-0.019787	2.507838
99.264056	2028.363151	5.502438	-0.019820	2.512432
99.476023	2036.412606	5.507443	-0.019865	2.516974
99.754136	2044.437366	5.512448	-0.019922	2.521500
99.983706	2052.485735	5.517453	-0.019970	2.526027
100.402327	2060.510261	5.522458	-0.020053	2.530546
100.597891	2068.611193	5.527462	-0.020095	2.535084
100.756966	2076.626317	5.532467	-0.020130	2.539563
101.162814	2084.666386	5.537472	-0.020211	2.544065
101.522666	2092.728496	5.542477	-0.020283	2.548569
101.751228	2100.785983	5.547482	-0.020331	2.553053
102.111942	2108.852603	5.552486	-0.020404	2.557543
102.218282	2116.891177	5.557491	-0.020429	2.561992
102.440617	2124.952083	5.562496	-0.020476	2.566453
102.814155	2133.012904	5.567501	-0.020551	2.570917
102.964761	2141.088206	5.572506	-0.020584	2.575366
103.450201	2149.127762	5.577510	-0.020680	2.579811
103.619876	2157.155258	5.582515	-0.020717	2.584219
103.908638	2165.226785	5.587520	-0.020776	2.588652
104.168341	2173.447925	5.592525	-0.020830	2.593158
104.428409	2181.472742	5.597530	-0.020884	2.597548
104.689570	2189.471819	5.602534	-0.020938	2.601917
105.147741	2197.459953	5.607539	-0.021029	2.606286
105.347515	2205.512372	5.612544	-0.021071	2.610665
105.674373	2213.566115	5.617549	-0.021138	2.615046
105.749712	2221.583231	5.622554	-0.021157	2.619383
106.263996	2229.617248	5.627558	-0.021258	2.623751
106.399750	2237.674934	5.632563	-0.021289	2.628100
106.720874	2245.735084	5.637568	-0.021354	2.632455
106.772128	2253.806827	5.642573	-0.021369	2.636790
106.892519	2261.837613	5.647578	-0.021397	2.641102
107.162588	2269.881316	5.652582	-0.021452	2.645423
107.490243	2277.909337	5.657587	-0.021519	2.649732
107.709770	2285.980866	5.662592	-0.021565	2.654050
107.671382	2294.050267	5.667597	-0.021563	2.658344
107.947318	2302.075510	5.672602	-0.021620	2.662627
108.553763	2310.114776	5.677606	-0.021738	2.666932
108.623000	2318.198572	5.682611	-0.021757	2.671219
108.862855	2326.281762	5.687616	-0.021807	2.675510
109.072657	2334.305989	5.692621	-0.021851	2.679761
109.271024	2342.307732	5.697626	-0.021894	2.683993
109.728790	2350.355557	5.702630	-0.021984	2.688258
109.804459	2358.431655	5.707635	-0.022004	2.692508
110.270882	2366.472276	5.712640	-0.022096	2.696757
110.455849	2374.526329	5.717645	-0.022136	2.700988
110.591419	2382.557848	5.722650	-0.022166	2.705197
110.920305	2390.612279	5.727654	-0.022233	2.709425
111.075952	2398.690047	5.732659	-0.022267	2.713647
111.208423	2406.727452	5.737664	-0.022298	2.717839
111.424700	2414.761942	5.742669	-0.022343	2.722029
111.608173	2422.759880	5.747674	-0.022383	2.726192
111.790134	2430.830625	5.752678	-0.022422	2.730386
112.035334	2438.872565	5.757683	-0.022473	2.734562
112.300028	2446.913752	5.762688	-0.022528	2.738733
112.513484	2454.957069	5.767693	-0.022573	2.742895
112.780517	2462.973645	5.772698	-0.022628	2.747040
113.116805	2471.065398	5.777702	-0.022696	2.751222
113.115644	2479.194813	5.782707	-0.022701	2.755397
113.416374	2487.206000	5.787712	-0.022763	2.759523
113.777701	2495.179520	5.792717	-0.022835	2.763626
113.973271	2503.213260	5.797722	-0.022877	2.767745
114.220749	2511.278106	5.802726	-0.022929	2.771876
114.489978	2519.314585	5.807731	-0.022984	2.775988
114.815245	2527.355377	5.812736	-0.023050	2.780100
115.041306	2535.367553	5.817741	-0.023098	2.784184
115.218521	2543.420707	5.822746	-0.023136	2.788281
115.530834	2551.502201	5.827750	-0.023200	2.792394
115.553030	2559.575058	5.832755	-0.023209	2.796480
115.844758	2567.579711	5.837760	-0.023269	2.800540
116.114677	2575.576373	5.842765	-0.023324	2.804590
116.246289	2583.638530	5.847770	-0.023354	2.808658
116.606052	2591.703598	5.852774	-0.023427	2.812736
116.792344	2599.734566	5.857779	-0.023467	2.816780
117.123104	2607.769964	5.862784	-0.023534	2.820829
117.309594	2615.815524	5.867789	-0.023574	2.824869
117.223956	2623.888820	5.872794	-0.023563	2.828901
117.631833	2631.968592	5.877798	-0.023645	2.832959
117.828891	2639.992720	5.882803	-0.023687	2.836972
118.031873	2648.015730	5.887808	-0.023730	2.840978
118.342867	2656.009650	5.892813	-0.023793	2.844970
118.598065	2664.028221	5.897818	-0.023846	2.848966
118.720625	2672.120460	5.902822	-0.023874	2.852986
118.856714	2680.160821	5.907827	-0.023905	2.856974
119.345305	2688.177819	5.912832	-0.024001	2.860965
119.684938	2696.197108	5.917837	-0.024070	2.864944
119.721944	2704.249061	5.922842	-0.024082	2.868916
120.297901	2712.297448	5.927846	-0.024195	2.872911
120.408752	2720.355418	5.932851	-0.024221	2.876879
120.521014	2728.395790	5.937856	-0.024247	2.880833
120.923593	2736.383671	5.942861	-0.024328	2.884771
121.068376	2744.455427	5.947866	-0.024360	2.888732
121.447879	2752.520561	5.952870	-0.024436	2.892696
121.310902	2760.594786	5.957875	-0.024416	2.896631
121.761924	2768.608382	5.962880	-0.024505	2.900563
121.919942	2776.641127	5.967885	-0.024540	2.904484
121.836141	2784.713438	5.972890	-0.024530	2.908405
122.244882	2792.800871	5.977894	-0.024612	2.912355
122.364442	2800.866905	5.982899	-0.024639	2.916273
122.623261	2808.842783	5.987904	-0.024693	2.920150
122.718643	2816.851841	5.992909	-0.024716	2.924029
123.002358	2824.843873	5.997914	-0.024774	2.927905
123.326801	2832.884299	6.002918	-0.024840	2.931801
123.605760	2840.947694	6.007923	-0.024897	2.935700
123.791801	2848.964549	6.012928	-0.024937	2.939567
124.127815	2856.977076	6.017933	-0.025005	2.943434
124.220506	2865.021505	6.022938	-0.025028	2.947299
124.496486	2873.086699	6.027942	-0.025085	2.951179
124.578365	2881.158828	6.032947	-0.025105	2.955046
124.765033	2889.160999	6.037952	-0.025145	2.958881
124.888774	2897.200065	6.042957	-0.025174	2.962725
125.179741	2905.231018	6.047962	-0.025233	2.966568
125.574475	2913.267323	6.052966	-0.025312	2.970414
125.653380	2921.324425	6.057971	-0.025332	2.974250
125.884215	2929.361265	6.062976	-0.025381	2.978078
126.208855	2937.393957	6.067981	-0.025447	2.981904
126.198743	2945.412112	6.072986	-0.025450	2.985701
126.481927	2953.458831	6.077990	-0.025508	2.989522
126.720675	2961.514104	6.082995	-0.025558	2.993339
126.979760	2969.548507	6.088000	-0.025612	2.997143
127.143548	2977.586762	6.093005	-0.025648	3.000939
127.387045	2985.557843	6.098010	-0.025698	3.004703
127.632040	2993.631942	6.103014	-0.025749	3.008510
127.663226	3001.684979	6.108019	-0.025761	3.012292
127.949953	3009.730009	6.113024	-0.025819	3.016078
128.163574	3017.752266	6.118029	-0.025865	3.019845
128.246911	3025.770891	6.123034	-0.025885	3.023599
128.661586	3033.817127	6.128038	-0.025968	3.027378
128.705318	3041.863389	6.133043	-0.025982	3.031134
128.814527	3049.930287	6.138048	-0.026007	3.034898
129.138445	3057.925909	6.143053	-0.026073	3.038634
129.435433	3065.920893	6.148058	-0.026134	3.042364
129.893911	3073.971071	6.153062	-0.026224	3.046123
129.835792	3082.011294	6.158067	-0.026219	3.049848
130.080276	3090.063217	6.163072	-0.026270	3.053588
130.380388	3098.093762	6.168077	-0.026331	3.057316
130.641809	3106.115923	6.173082	-0.026385	3.061034
130.895313	3114.139310	6.178086	-0.026438	3.064748
131.146742	3122.175491	6.183091	-0.026490	3.068463
131.230968	3130.303087	6.188096	-0.026511	3.072207
131.311761	3138.378477	6.193101	-0.026532	3.075923
131.746505	3146.312042	6.198106	-0.026618	3.079586
131.894648	3154.344296	6.203110	-0.026651	3.083276
132.108253	3162.359851	6.208115	-0.026696	3.086957
132.186172	3170.399482	6.213120	-0.026716	3.090639
132.606238	3178.462103	6.218125	-0.026800	3.094342
132.669287	3186.457593	6.223130	-0.026817	3.097994
132.918152	3194.515164	6.228134	-0.026868	3.101678
132.999883	3202.520986	6.233139	-0.026889	3.105327
133.269326	3210.567638	6.238144	-0.026945	3.108998
133.534338	3218.626452	6.243149	-0.026999	3.112671
133.788383	3226.637489	6.248154	-0.027052	3.116317
133.930874	3234.682929	6.253158	-0.027084	3.119969
134.003943	3242.689553	6.258163	-0.027103	3.123596
134.226682	3250.719027	6.263168	-0.027150	3.127236
134.637174	3258.781611	6.268173	-0.027232	3.130895
134.714936	3266.809800	6.273178	-0.027252	3.134519
134.896318	3274.847521	6.278182	-0.027291	3.138148
134.946102	3282.879120	6.283187	-0.027305	3.141764
135.298830	3290.869431	6.288192	-0.027376	3.145371
135.391296	3298.929374	6.293197	-0.027399	3.148994
135.611492	3306.981990	6.298202	-0.027445	3.152614
135.857761	3315.070034	6.303206	-0.027497	3.156248
135.874333	3323.032083	6.308211	-0.027505	3.159810
136.027799	3331.059040	6.313216	-0.027539	3.163404
136.404576	3339.079860	6.318221	-0.027615	3.167001
136.407912	3347.095677	6.323226	-0.027621	3.170575
136.627031	3355.167752	6.328230	-0.027667	3.174179
136.891338	3363.177351	6.333235	-0.027721	3.177754
137.114836	3371.207062	6.338240	-0.027768	3.181331
137.403168	3379.216482	6.343245	-0.027828	3.184898
137.685805	3387.243329	6.348250	-0.027886	3.188469
138.161106	3395.292651	6.353254	-0.027979	3.192054
137.972555	3403.397636	6.358259	-0.027950	3.195631
138.131991	3411.358306	6.363264	-0.027985	3.199155
138.583005	3419.381534	6.368269	-0.028074	3.202715
138.620840	3427.421204	6.373274	-0.028087	3.206261
138.717871	3435.464200	6.378278	-0.028110	3.209807
138.960164	3443.509533	6.383283	-0.028161	3.213356
139.236820	3451.535057	6.388288	-0.028217	3.216894
139.462085	3459.565140	6.393293	-0.028265	3.220428
139.657556	3467.559933	6.398298	-0.028307	3.223941
139.920580	3475.632831	6.403302	-0.028361	3.227487
140.337047	3483.649711	6.408307	-0.028444	3.231011
140.484398	3491.743539	6.413312	-0.028477	3.234554
140.574582	3499.737140	6.418317	-0.028499	3.238047
140.651567	3507.751395	6.423322	-0.028519	3.241544
141.181053	3515.727403	6.428326	-0.028623	3.245040
141.503364	3523.744356	6.433331	-0.028688	3.248541
141.699422	3531.810521	6.438336	-0.028730	3.252054
141.996169	3539.866890	6.443341	-0.028791	3.255564
141.965544	3547.881508	6.448346	-0.028790	3.259038
142.261660	3555.886252	6.453350	-0.028851	3.262518
142.385042	3563.915496	6.458355	-0.028879	3.265997
142.627265	3571.951193	6.463360	-0.028930	3.269480
142.791298	3580.028026	6.468365	-0.028966	3.272975
142.820409	3588.056322	6.473370	-0.028976	3.276439
143.143324	3596.057787	6.478374	-0.029042	3.279899
143.445230	3604.069768	6.483379	-0.029103	3.283360
143.604825	3612.101029	6.488384	-0.029139	3.286819
143.707403	3620.138703	6.493389	-0.029163	3.290275
143.719706	3628.193731	6.498394	-0.029171	3.293732
144.103741	3636.225336	6.503398	-0.029248	3.297189
144.227143	3644.234185	6.508403	-0.029276	3.300623
144.394738	3652.236538	6.513408	-0.029313	3.304053
144.667192	3660.298623	6.518413	-0.029369	3.307508
144.912268	3668.342440	6.523418	-0.029420	3.310950
145.164201	3676.399274	6.528422	-0.029472	3.314395
145.213965	3684.402588	6.533427	-0.029487	3.317806
145.435558	3692.411464	6.538432	-0.029533	3.321222
145.736450	3700.395252	6.543437	-0.029595	3.324627
145.850408	3708.403822	6.548442	-0.029621	3.328032
146.201291	3716.464659	6.553446	-0.029692	3.331464
146.443982	3724.519874	6.558451	-0.029743	3.334886
146.461182	3732.538257	6.563456	-0.029751	3.338281
146.624148	3740.583132	6.568461	-0.029787	3.341689
146.813168	3748.568229	6.573466	-0.029827	3.345069
147.112992	3756.647363	6.578470	-0.029889	3.348490
147.225100	3764.671889	6.583475	-0.029915	3.351877
147.515511	3772.723301	6.588480	-0.029974	3.355278
147.887213	3780.727018	6.593485	-0.030049	3.358659
147.984384	3788.718755	6.598490	-0.030073	3.362022
148.301983	3796.738308	6.603494	-0.030137	3.365400
148.517181	3804.766658	6.608499	-0.030182	3.368775
148.617615	3812.836830	6.613504	-0.030207	3.372161
148.886290	3820.900823	6.618509	-0.030262	3.375546
149.057068	3828.869332	6.623514	-0.030299	3.378884
149.411653	3836.898250	6.628518	-0.030371	3.382251
149.478898	3844.933477	6.633523	-0.030389	3.385607
149.838624	3852.952757	6.638528	-0.030461	3.388963
150.197827	3861.043205	6.643533	-0.030533	3.392345
150.259329	3869.087363	6.648538	-0.030550	3.395695
150.432059	3877.115892	6.653542	-0.030588	3.399038
150.809368	3885.078127	6.658547	-0.030663	3.402358
150.808908	3893.093419	6.663552	-0.030668	3.405683
151.024270	3901.123443	6.668557	-0.030714	3.409018
151.276703	3909.131202	6.673562	-0.030766	3.412343
151.489583	3917.174339	6.678566	-0.030811	3.415677
151.653106	3925.183418	6.683571	-0.030847	3.418992
151.744371	3933.216154	6.688576	-0.030870	3.422312
152.093788	3941.239271	6.693581	-0.030940	3.425632
152.048233	3949.264124	6.698586	-0.030937	3.428937
152.579944	3957.323009	6.703590	-0.031041	3.432273
152.745359	3965.360688	6.708595	-0.031078	3.435583
152.736788	3973.350447	6.713600	-0.031081	3.438866
153.074879	3981.383564	6.718605	-0.031150	3.442174
153.126683	3989.410486	6.723610	-0.031165	3.445467
153.539831	3997.428823	6.728614	-0.031247	3.448766
153.681617	4005.476956	6.733619	-0.031279	3.452064
153.765571	4013.521476	6.738624	-0.031300	3.455356
154.127718	4021.545235	6.743629	-0.031373	3.458645
154.191225	4029.559424	6.748634	-0.031390	3.461918
154.464805	4037.576686	6.753638	-0.031446	3.465195
154.660460	4045.608658	6.758643	-0.031488	3.468473
154.783435	4053.679443	6.763648	-0.031516	3.471761
154.824326	4061.736803	6.768653	-0.031529	3.475038
155.020311	4069.677994	6.773658	-0.031571	3.478269
155.184721	4077.744630	6.778662	-0.031607	3.481548
155.341445	4085.697819	6.783667	-0.031642	3.484777
155.500664	4093.735391	6.788672	-0.031677	3.488037
155.839448	4101.791182	6.793677	-0.031745	3.491308
155.724164	4109.812950	6.798682	-0.031729	3.494547
156.170360	4117.839282	6.803686	-0.031818	3.497802
156.407484	4125.857070	6.808691	-0.031867	3.501045
156.574462	4133.852212	6.813696	-0.031904	3.504273
156.684494	4141.919716	6.818701	-0.031929	3.507525
156.791111	4149.907310	6.823706	-0.031955	3.510743
156.904154	4157.986485	6.828710	-0.031981	3.513994
157.058147	4166.001614	6.833715	-0.032015	3.517218
157.255619	4174.004494	6.838720	-0.032057	3.520435
157.575844	4182.014753	6.843725	-0.032122	3.523656
157.632982	4190.022153	6.848730	-0.032138	3.526865
157.834888	4198.094553	6.853734	-0.032181	3.530101
158.009594	4206.127304	6.858739	-0.032219	3.533317
158.314821	4214.174785	6.863744	-0.032282	3.536541
158.449776	4222.194868	6.868749	-0.032312	3.539745
158.363785	4230.204457	6.873754	-0.032301	3.542936
158.918944	4238.199728	6.878758	-0.032410	3.546137
158.893300	4246.250715	6.883763	-0.032411	3.549341
159.183590	4254.340350	6.888768	-0.032470	3.552566
159.226188	4262.418984	6.893773	-0.032484	3.555776
159.511807	4270.338920	6.898778	-0.032542	3.558928
159.454313	4278.391496	6.903782	-0.032537	3.562119
159.492926	4286.366113	6.908787	-0.032549	3.565279
159.885263	4294.372241	6.913792	-0.032628	3.568460
160.117913	4302.436937	6.918797	-0.032676	3.571656
160.274644	4310.418095	6.923802	-0.032711	3.574814
160.476624	4318.461630	6.928806	-0.032754	3.577995
160.531850	4326.502542	6.933811	-0.032770	3.581167
160.686208	4334.491880	6.938816	-0.032804	3.584320
160.990652	4342.538520	6.943821	-0.032866	3.587497
161.142447	4350.530438	6.948826	-0.032900	3.590645
161.263161	4358.611165	6.953830	-0.032927	3.593824
161.325550	4366.634104	6.958835	-0.032944	3.596976
161.551470	4374.600621	6.963840	-0.032992	3.600107
161.856662	4382.613129	6.968845	-0.033054	3.603257
161.787338	4390.621262	6.973850	-0.033047	3.606391
162.311354	4398.655536	6.978854	-0.033149	3.609549
162.371459	4406.694893	6.983859	-0.033166	3.612693
162.246994	4414.742370	6.988864	-0.033148	3.615833
162.683681	4422.745942	6.993869	-0.033235	3.618969
162.941412	4430.755649	6.998874	-0.033288	3.622099
163.067734	4438.794470	7.003878	-0.033317	3.625234
163.204318	4446.817127	7.008883	-0.033348	3.628360
163.411896	4454.893212	7.013888	-0.033392	3.631507
163.557446	4462.943748	7.018893	-0.033425	3.634639
163.593710	4470.953381	7.023898	-0.033437	3.637749
163.991898	4478.968167	7.028902	-0.033516	3.640869
164.140121	4486.954899	7.033907	-0.033549	3.643968
164.293989	4494.956988	7.038912	-0.033583	3.647070
164.621173	4503.011378	7.043917	-0.033650	3.650195
164.693702	4511.045023	7.048922	-0.033668	3.653303
164.855297	4519.103724	7.053926	-0.033704	3.656419
165.161922	4527.062374	7.058931	-0.033766	3.659499
165.305745	4535.101306	7.063936	-0.033799	3.662602
165.552865	4543.133645	7.068941	-0.033850	3.665703
165.751018	4551.129145	7.073946	-0.033892	3.668785
165.896869	4559.202396	7.078950	-0.033925	3.671894
166.085233	4567.225247	7.083955	-0.033965	3.674981
166.200994	4575.205291	7.088960	-0.033992	3.678048
166.282525	4583.301814	7.093965	-0.034013	3.681156
166.345290	4591.224752	7.098970	-0.034030	3.684195
166.517365	4599.301968	7.103974	-0.034067	3.687292
166.689015	4607.294668	7.108979	-0.034105	3.690355
166.924474	4615.338897	7.113984	-0.034154	3.693436
167.083921	4623.397410	7.118989	-0.034189	3.696519
167.240072	4631.364746	7.123994	-0.034223	3.699564
167.391269	4639.422583	7.128998	-0.034257	3.702640
167.612535	4647.408858	7.134003	-0.034303	3.705689
167.726320	4655.433413	7.139008	-0.034330	3.708747
167.785774	4663.538778	7.144013	-0.034347	3.711832
167.978346	4671.575760	7.149018	-0.034388	3.714891
168.255445	4679.564671	7.154022	-0.034445	3.717932
168.243594	4687.555765	7.159027	-0.034448	3.720964
168.534537	4695.507629	7.164032	-0.034507	3.723986
168.725570	4703.568924	7.169037	-0.034548	3.727045
168.748704	4711.560983	7.174042	-0.034558	3.730071
169.002319	4719.627502	7.179046	-0.034611	3.733128
169.249961	4727.663941	7.184051	-0.034662	3.736171
169.423497	4735.638107	7.189056	-0.034700	3.739186
169.495858	4743.686411	7.194061	-0.034719	3.742224
169.685639	4751.685884	7.199066	-0.034759	3.745245
169.707965	4759.777820	7.204070	-0.034769	3.748293
169.544327	4767.797494	7.209075	-0.034744	3.751308
169.755175	4775.796150	7.214080	-0.034789	3.754321
170.086769	4783.825442	7.219085	-0.034856	3.757346
169.995427	4791.821738	7.224090	-0.034844	3.760346
170.250412	4799.848874	7.229094	-0.034897	3.763364
170.526198	4807.857133	7.234099	-0.034954	3.766372
170.554222	4815.877895	7.239104	-0.034964	3.769377
170.643043	4823.961457	7.244109	-0.034986	3.772404
170.757171	4831.958988	7.249114	-0.035013	3.775398
171.053739	4839.987821	7.254118	-0.035073	3.778404
171.084132	4848.016662	7.259123	-0.035084	3.781403
171.226492	4855.957257	7.264128	-0.035116	3.784368
171.482973	4864.065715	7.269133	-0.035170	3.787397
171.399502	4872.047649	7.274138	-0.035159	3.790368
171.634157	4880.164564	7.279142	-0.035208	3.793394
172.196321	4888.134251	7.284147	-0.035318	3.796370
172.118860	4896.109629	7.289152	-0.035309	3.799332
172.237065	4904.136022	7.294157	-0.035337	3.802315
172.334526	4912.097599	7.299162	-0.035360	3.805271
172.819739	4920.158961	7.304166	-0.035456	3.808270
172.857155	4928.194868	7.309171	-0.035468	3.811247
173.256665	4936.210102	7.314176	-0.035548	3.814223
173.405820	4944.248831	7.319181	-0.035581	3.817199
173.427548	4952.242112	7.324186	-0.035591	3.820153
173.579754	4960.258609	7.329190	-0.035624	3.823116
173.923818	4968.272921	7.334195	-0.035694	3.826081
174.079507	4976.297609	7.339200	-0.035728	3.829043
174.250055	4984.369279	7.344205	-0.035765	3.832020
174.232884	4992.372284	7.349210	-0.035768	3.834965
174.364594	5000.395085	7.354214	-0.035798	3.837919
174.307752	5008.437324	7.359219	-0.035792	3.840874
174.554100	5016.357279	7.364224	-0.035844	3.843788
174.644079	5024.461485	7.369229	-0.035866	3.846763
174.767238	5032.423662	7.374234	-0.035894	3.849686
175.078693	5040.484604	7.379238	-0.035957	3.852646
175.293735	5048.546148	7.384243	-0.036003	3.855602
175.580398	5056.519527	7.389248	-0.036062	3.858524
175.531283	5064.626082	7.394253	-0.036058	3.861487
175.734333	5072.565976	7.399258	-0.036101	3.864391
176.103691	5080.602953	7.404262	-0.036175	3.867332
176.141448	5088.627465	7.409267	-0.036188	3.870260
176.192646	5096.842453	7.414272	-0.036203	3.873255
176.685741	5104.878684	7.419277	-0.036300	3.876191
176.617586	5112.762665	7.424282	-0.036292	3.879058
176.488469	5120.806903	7.429286	-0.036274	3.881981
176.889079	5128.702442	7.434291	-0.036354	3.884858
177.052467	5136.746556	7.439296	-0.036390	3.887781
177.130928	5144.810786	7.444301	-0.036410	3.890708
177.165161	5152.801628	7.449306	-0.036421	3.893606
177.417431	5160.867123	7.454310	-0.036474	3.896533
177.624152	5168.832478	7.459315	-0.036518	3.899420
177.516023	5176.860901	7.464320	-0.036503	3.902322
177.890184	5184.861460	7.469325	-0.036578	3.905220
177.996299	5192.902816	7.474330	-0.036603	3.908127
177.918139	5200.920810	7.479334	-0.036594	3.911019
177.866601	5208.952001	7.484339	-0.036590	3.913914
178.046736	5216.960751	7.489344	-0.036628	3.916804
178.182957	5224.993360	7.494349	-0.036659	3.919699
178.238058	5232.957994	7.499354	-0.036675	3.922566
178.359834	5240.985899	7.504358	-0.036703	3.925454
178.557712	5249.026357	7.509363	-0.036745	3.928347
178.736885	5257.047679	7.514368	-0.036784	3.931230
179.106149	5265.096766	7.519373	-0.036858	3.934125
179.031356	5273.099242	7.524378	-0.036849	3.936992
179.262697	5281.100117	7.529382	-0.036898	3.939863
179.427797	5289.118945	7.534387	-0.036934	3.942736
179.743141	5297.124048	7.539392	-0.036998	3.945605
179.723777	5305.169954	7.544397	-0.037000	3.948481
179.759002	5313.195439	7.549402	-0.037012	3.951348
180.088751	5321.231634	7.554406	-0.037079	3.954222
180.142870	5329.240829	7.559411	-0.037094	3.957080
180.253043	5337.211942	7.564416	-0.037120	3.959923
180.521456	5345.264504	7.569421	-0.037175	3.962795
180.512419	5353.256514	7.574426	-0.037179	3.965639
180.641543	5361.281020	7.579430	-0.037208	3.968495
180.854205	5369.315293	7.584435	-0.037253	3.971354
181.018404	5377.326095	7.589440	-0.037289	3.974202
181.172641	5385.398637	7.594445	-0.037324	3.977069
181.205198	5393.363031	7.599450	-0.037335	3.979894
181.504552	5401.404316	7.604454	-0.037396	3.982748
181.695602	5409.434514	7.609459	-0.037437	3.985595
181.573618	5417.450685	7.614464	-0.037420	3.988429
181.940464	5425.475478	7.619469	-0.037493	3.991273
182.432982	5433.489752	7.624474	-0.037590	3.994113
182.309094	5441.563033	7.629478	-0.037573	3.996961
182.540405	5449.527525	7.634483	-0.037621	3.999775
182.687026	5457.537906	7.639488	-0.037654	4.002602
182.962546	5465.558808	7.644493	-0.037711	4.005432
183.049980	5473.559408	7.649498	-0.037732	4.008250
183.330584	5481.587177	7.654502	-0.037790	4.011079
183.481370	5489.654089	7.659507	-0.037823	4.013918
183.615804	5497.707067	7.664512	-0.037854	4.016749
183.832042	5505.692773	7.669517	-0.037899	4.019556
183.959633	5513.702320	7.674522	-0.037929	4.022368
183.877499	5521.743686	7.679526	-0.037919	4.025186
184.101836	5529.780802	7.684531	-0.037966	4.028005
184.264130	5537.755882	7.689536	-0.038001	4.030800
184.614148	5545.895358	7.694541	-0.038072	4.033652
184.698227	5553.885190	7.699546	-0.038093	4.036447
185.077347	5561.801755	7.704550	-0.038169	4.039218
185.055408	5569.864552	7.709555	-0.038170	4.042033
184.897803	5577.814318	7.714560	-0.038146	4.044804
185.347044	5585.853907	7.719565	-0.038235	4.047613
185.609534	5593.858759	7.724570	-0.038290	4.050406
185.811555	5601.935489	7.729574	-0.038333	4.053221
185.833684	5609.952742	7.734579	-0.038342	4.056010
185.944748	5617.912536	7.739584	-0.038368	4.058779
186.273032	5625.970392	7.744589	-0.038435	4.061583
186.109387	5633.950816	7.749594	-0.038410	4.064352
186.375941	5641.991861	7.754598	-0.038465	4.067145
186.586919	5650.002092	7.759603	-0.038509	4.069925
186.638478	5658.031593	7.764608	-0.038524	4.072708
186.963437	5666.059152	7.769613	-0.038590	4.075492
187.003906	5674.019861	7.774618	-0.038603	4.078247
187.113849	5682.049129	7.779622	-0.038629	4.081024
187.302116	5690.047351	7.784627	-0.038669	4.083791
187.432040	5698.101338	7.789632	-0.038699	4.086573
187.598994	5706.096053	7.794637	-0.038735	4.089334
187.694277	5714.137109	7.799642	-0.038758	4.092108
187.835444	5722.186404	7.804646	-0.038790	4.094883
188.207665	5730.195043	7.809651	-0.038865	4.097646
188.221745	5738.184098	7.814656	-0.038873	4.100395
188.349317	5746.247719	7.819661	-0.038902	4.103170
188.773054	5754.193712	7.824666	-0.038986	4.105906
188.822555	5762.268604	7.829670	-0.039001	4.108680
189.046398	5770.330530	7.834675	-0.039048	4.111449
189.300682	5778.359506	7.839680	-0.039101	4.114206
189.311451	5786.381259	7.844685	-0.039108	4.116955
189.229942	5794.307879	7.849690	-0.039098	4.119669
189.383191	5802.397045	7.854694	-0.039132	4.122439
189.583596	5810.407799	7.859699	-0.039175	4.125181
189.850621	5818.393196	7.864704	-0.039230	4.127914
189.913034	5826.439038	7.869709	-0.039247	4.130663
190.175660	5834.457365	7.874714	-0.039301	4.133403
190.292122	5842.506566	7.879718	-0.039328	4.136150
190.310716	5850.485907	7.884723	-0.039337	4.138871
190.472712	5858.508463	7.889728	-0.039373	4.141605
190.712664	5866.504263	7.894733	-0.039423	4.144330
190.782865	5874.544496	7.899738	-0.039441	4.147066
191.065153	5882.592705	7.904742	-0.039499	4.149806
191.234531	5890.635607	7.909747	-0.039536	4.152541
191.287536	5898.629995	7.914752	-0.039551	4.155255
191.526333	5906.652655	7.919757	-0.039601	4.157980
191.780957	5914.636849	7.924762	-0.039654	4.160691
191.877657	5922.665875	7.929766	-0.039677	4.163412
192.012391	5930.711818	7.934771	-0.039708	4.166138
192.256640	5938.673556	7.939776	-0.039759	4.168836
192.701538	5946.700290	7.944781	-0.039847	4.171555
192.595591	5954.756445	7.949786	-0.039833	4.174277
192.538122	5962.764426	7.954790	-0.039827	4.176981
192.772987	5970.761425	7.959795	-0.039876	4.179682
192.908898	5978.789181	7.964800	-0.039907	4.182392
193.203792	5986.798475	7.969805	-0.039967	4.185095
193.340379	5994.786702	7.974810	-0.039998	4.187787
193.503812	6002.851627	7.979814	-0.040034	4.190504
193.587847	6010.969898	7.984819	-0.040055	4.193236
193.504265	6018.983674	7.989824	-0.040045	4.195929
193.911173	6026.913573	7.994829	-0.040126	4.198598
193.962130	6034.886893	7.999834	-0.040141	4.201276
193.977098	6042.880417	8.004838	-0.040149	4.203958
194.268334	6050.935643	8.009843	-0.040209	4.206662
194.258948	6058.892728	8.014848	-0.040212	4.209329
194.524238	6066.991880	8.019853	-0.040267	4.212044
194.517645	6074.974053	8.024858	-0.040271	4.214716
194.710278	6083.004729	8.029862	-0.040312	4.217404
194.838245	6090.996786	8.034867	-0.040342	4.220076
195.121877	6099.005194	8.039872	-0.040400	4.222754
195.416159	6107.032525	8.044877	-0.040460	4.225437
195.539194	6115.041136	8.049882	-0.040488	4.228110
195.602657	6123.112826	8.054886	-0.040505	4.230802
195.828493	6131.118400	8.059891	-0.040553	4.233472
195.962001	6139.143998	8.064896	-0.040583	4.236145
196.011819	6147.124586	8.069901	-0.040598	4.238801
196.190514	6155.162863	8.074906	-0.040636	4.241476
196.407662	6163.098079	8.079910	-0.040682	4.244116
196.525550	6171.230125	8.084915	-0.040710	4.246818
196.541863	6179.157622	8.089920	-0.040718	4.249449
196.813050	6187.256174	8.094925	-0.040774	4.252138
196.862948	6195.277538	8.099930	-0.040789	4.254798
197.124754	6203.290589	8.104934	-0.040843	4.257455
197.175773	6211.294700	8.109939	-0.040858	4.260106
197.541309	6219.282096	8.114944	-0.040931	4.262752
197.530092	6227.309292	8.119949	-0.040934	4.265406
197.444523	6235.344420	8.124954	-0.040924	4.268061
197.921031	6243.355452	8.129958	-0.041018	4.270711
198.061546	6251.467545	8.134963	-0.041049	4.273390
198.175857	6259.446299	8.139968	-0.041076	4.276022
198.529350	6267.446566	8.144973	-0.041147	4.278663
198.500986	6275.443731	8.149978	-0.041147	4.281297
198.503273	6283.452624	8.154982	-0.041153	4.283934
198.736427	6291.500478	8.159987	-0.041202	4.286584
198.720748	6299.462795	8.164992	-0.041204	4.289202
198.980608	6307.571357	8.169997	-0.041258	4.291869
199.183519	6315.532438	8.175002	-0.041301	4.294485
199.428710	6323.595429	8.180006	-0.041352	4.297133
199.363650	6331.552997	8.185011	-0.041346	4.299743
199.435772	6339.587327	8.190016	-0.041364	4.302377
199.760433	6347.610083	8.195021	-0.041430	4.305008
199.911659	6355.629607	8.200026	-0.041464	4.307635
200.080158	6363.635554	8.205030	-0.041501	4.310256
199.860561	6371.673666	8.210035	-0.041465	4.312883
200.100236	6379.669640	8.215040	-0.041515	4.315498
200.390397	6387.699049	8.220045	-0.041574	4.318123
200.252424	6395.683907	8.225050	-0.041554	4.320728
200.446809	6403.704319	8.230054	-0.041596	4.323346
200.533892	6411.737830	8.235059	-0.041617	4.325965
200.583558	6419.720533	8.240064	-0.041632	4.328567
201.022419	6427.787734	8.245069	-0.041719	4.331197
201.103276	6435.773786	8.250074	-0.041739	4.333796
201.333485	6443.866112	8.255078	-0.041788	4.336429
201.394566	6451.821034	8.260083	-0.041804	4.339015
201.394210	6459.821456	8.265088	-0.041810	4.341614
201.629645	6467.835185	8.270093	-0.041859	4.344217
201.630746	6475.876036	8.275098	-0.041865	4.346826
201.936378	6483.848978	8.280102	-0.041927	4.349413
202.121043	6491.989253	8.285107	-0.041967	4.352052
202.086601	6500.012664	8.290112	-0.041966	4.354650
202.397916	6508.031029	8.295117	-0.042029	4.357247
202.583652	6515.947705	8.300122	-0.042069	4.359809
202.502177	6523.980645	8.305126	-0.042059	4.362406
202.660915	6531.953733	8.310131	-0.042094	4.364983
202.911027	6539.995612	8.315136	-0.042146	4.367581
203.240036	6548.018622	8.320141	-0.042213	4.370172
203.353882	6556.063189	8.325146	-0.042239	4.372767
203.273816	6564.067767	8.330150	-0.042230	4.375346
203.356823	6572.045910	8.335155	-0.042251	4.377916
203.515054	6580.066209	8.340160	-0.042285	4.380499
203.811249	6588.108225	8.345165	-0.042346	4.383088
203.930363	6596.084483	8.350170	-0.042373	4.385654
203.997199	6604.094576	8.355174	-0.042391	4.388228
203.990462	6612.151538	8.360179	-0.042395	4.390816
204.322192	6620.183064	8.365184	-0.042463	4.393395
204.681865	6628.210210	8.370189	-0.042535	4.395972
204.764874	6636.142676	8.375194	-0.042556	4.398516
204.736026	6644.252221	8.380198	-0.042556	4.401114
204.903857	6652.217006	8.385203	-0.042592	4.403665
204.957958	6660.235186	8.390208	-0.042608	4.406231
205.162246	6668.278099	8.395213	-0.042651	4.408805
205.417790	6676.257569	8.400218	-0.042704	4.411357
205.632155	6684.303027	8.405222	-0.042750	4.413928
205.379850	6692.355657	8.410227	-0.042708	4.416498
205.599803	6700.301869	8.415232	-0.042754	4.419034
206.049283	6708.403978	8.420237	-0.042843	4.421620
206.046548	6716.298319	8.425242	-0.042848	4.424136
206.146385	6724.377996	8.430246	-0.042872	4.426710
206.399627	6732.446447	8.435251	-0.042925	4.429280
206.289661	6740.490578	8.440256	-0.042910	4.431839
206.506165	6748.523873	8.445261	-0.042955	4.434394
206.742730	6756.506582	8.450266	-0.043005	4.436932
206.845195	6764.441741	8.455270	-0.043029	4.439453
207.037639	6772.522885	8.460275	-0.043070	4.442019
207.127235	6780.459556	8.465280	-0.043092	4.444537
207.490212	6788.583306	8.470285	-0.043165	4.447114
207.330901	6796.526563	8.475290	-0.043141	4.449631
207.585360	6804.561629	8.480294	-0.043194	4.452176
207.993737	6812.603400	8.485299	-0.043275	4.454723
207.894989	6820.623692	8.490304	-0.043262	4.457260
207.951533	6828.610065	8.495309	-0.043278	4.459785
208.068882	6836.619039	8.500314	-0.043305	4.462316
208.328008	6844.623016	8.505318	-0.043359	4.464844
208.379935	6852.731036	8.510323	-0.043374	4.467404
208.382573	6860.691831	8.515328	-0.043380	4.469915
208.624463	6868.747524	8.520333	-0.043430	4.472455
208.921512	6876.725018	8.525338	-0.043491	4.474969
208.811423	6884.767109	8.530342	-0.043476	4.477501
208.989068	6892.712391	8.535347	-0.043514	4.480002
209.261801	6900.728704	8.540352	-0.043571	4.482525
209.207419	6908.767932	8.545357	-0.043566	4.485052
209.338418	6916.791908	8.550362	-0.043596	4.487573
209.504965	6924.779325	8.555366	-0.043632	4.490081
209.597868	6932.856587	8.560371	-0.043655	4.492617
209.623040	6940.846504	8.565376	-0.043665	4.495123
209.910345	6948.868330	8.570381	-0.043724	4.497638
210.036354	6956.813512	8.575386	-0.043752	4.500127
210.128061	6964.858208	8.580391	-0.043775	4.502647
210.300290	6972.883795	8.585395	-0.043812	4.505159
210.423669	6980.899379	8.590400	-0.043841	4.507666
210.657809	6988.953519	8.595405	-0.043890	4.510184
210.884010	6997.008328	8.600410	-0.043937	4.512701
211.054321	7005.028172	8.605415	-0.043974	4.515205
211.200387	7013.028715	8.610419	-0.044007	4.517702
211.272663	7020.951204	8.615424	-0.044026	4.520174
211.618484	7029.021302	8.620429	-0.044095	4.522690
211.605372	7036.946266	8.625434	-0.044098	4.525159
211.454286	7044.994880	8.630439	-0.044076	4.527664
211.687743	7053.012156	8.635443	-0.044124	4.530160
211.810433	7061.074851	8.640448	-0.044153	4.532668
211.997319	7069.104483	8.645453	-0.044193	4.535164
212.133932	7077.088675	8.650458	-0.044224	4.537645
212.367385	7085.099843	8.655463	-0.044273	4.540133
212.548901	7093.121848	8.660467	-0.044312	4.542623
212.507300	7101.065022	8.665472	-0.044309	4.545086
212.902892	7109.159199	8.670477	-0.044388	4.547596
212.881813	7117.174535	8.675482	-0.044390	4.550079
212.766134	7125.174559	8.680487	-0.044374	4.552556
213.040622	7133.250658	8.685491	-0.044430	4.555056
213.205431	7141.285380	8.690496	-0.044466	4.557541
213.266825	7149.263406	8.695501	-0.044483	4.560008
213.274152	7157.231865	8.700506	-0.044490	4.562470
213.644558	7165.253709	8.705511	-0.044564	4.564947
213.738479	7173.339836	8.710515	-0.044587	4.567443
213.697928	7181.297295	8.715520	-0.044585	4.569898
214.127175	7189.394113	8.720525	-0.044670	4.572394
214.196059	7197.357884	8.725530	-0.044688	4.574848
214.280836	7205.398928	8.730535	-0.044710	4.577325
214.229134	7213.368675	8.735539	-0.044705	4.579778
214.406993	7221.387732	8.740544	-0.044744	4.582245
214.654682	7229.395773	8.745549	-0.044795	4.584707
214.748036	7237.471598	8.750554	-0.044818	4.587189
214.721411	7245.425000	8.755559	-0.044818	4.589631
214.951031	7253.498108	8.760563	-0.044867	4.592109
214.776453	7261.469515	8.765568	-0.044839	4.594555
215.045296	7269.571711	8.770573	-0.044895	4.597039
215.250161	7277.502206	8.775578	-0.044938	4.599470
215.507348	7285.506249	8.780583	-0.044992	4.601922
215.518229	7293.514916	8.785587	-0.044999	4.604373
215.568026	7301.534976	8.790592	-0.045014	4.606827
215.933933	7309.555062	8.795597	-0.045087	4.609280
215.881154	7317.570549	8.800602	-0.045083	4.611730
216.047521	7325.639307	8.805607	-0.045119	4.614195
216.178471	7333.669495	8.810611	-0.045149	4.616646
216.265796	7341.619062	8.815616	-0.045171	4.619072
216.556201	7349.660980	8.820621	-0.045230	4.621525
216.708482	7357.615013	8.825626	-0.045264	4.623949
216.800256	7365.670618	8.830631	-0.045286	4.626403
217.094905	7373.705097	8.835635	-0.045346	4.628850
217.314897	7381.744891	8.840640	-0.045393	4.631297
217.406255	7389.762165	8.845645	-0.045415	4.633735
217.421646	7397.791807	8.850650	-0.045423	4.636176
217.464964	7405.732219	8.855655	-0.045437	4.638589
217.751978	7413.822245	8.860659	-0.045496	4.641046
217.703125	7421.726662	8.865664	-0.045492	4.643445
217.995713	7429.781085	8.870669	-0.045552	4.645888
217.978439	7437.772150	8.875674	-0.045554	4.648311
218.284350	7445.830085	8.880679	-0.045616	4.650753
218.249668	7453.892427	8.885683	-0.045615	4.653195
218.622061	7461.840597	8.890688	-0.045690	4.655601
218.711027	7469.920079	8.895693	-0.045712	4.658045
218.798838	7477.902645	8.900698	-0.045734	4.660459
218.857114	7485.918213	8.905703	-0.045750	4.662882
219.061862	7493.904433	8.910707	-0.045793	4.665294
219.122900	7501.901531	8.915712	-0.045810	4.667709
219.342691	7509.961425	8.920717	-0.045856	4.670141
219.343952	7518.053631	8.925722	-0.045862	4.672582
219.602092	7526.115015	8.930727	-0.045916	4.675011
219.592587	7534.057108	8.935731	-0.045919	4.677404
219.972132	7541.997970	8.940736	-0.045995	4.679795
220.091788	7550.021577	8.945741	-0.046023	4.682210
219.961293	7557.943183	8.950746	-0.046004	4.684594
220.099901	7566.075928	8.955751	-0.046035	4.687039
220.473889	7574.062639	8.960755	-0.046110	4.689438
220.665023	7582.083684	8.965760	-0.046151	4.691847
220.644583	7590.126345	8.970765	-0.046153	4.694262
220.677598	7598.180775	8.975770	-0.046164	4.696678
220.889041	7606.065617	8.980775	-0.046209	4.699043
220.918110	7614.139764	8.985779	-0.046220	4.701463
221.176091	7622.096692	8.990784	-0.046273	4.703846
221.405131	7630.178528	8.995789	-0.046321	4.706266
221.329896	7638.172645	9.000794	-0.046312	4.708659
221.508575	7646.196738	9.005799	-0.046351	4.711058
221.677051	7654.246854	9.010803	-0.046388	4.713465
221.778562	7662.259870	9.015808	-0.046412	4.715859
221.903958	7670.267790	9.020813	-0.046441	4.718251
221.992967	7678.230359	9.025818	-0.046463	4.720627
222.235773	7686.233881	9.030823	-0.046513	4.723015
222.659139	7694.326903	9.035827	-0.046598	4.725427
222.773320	7702.335561	9.040832	-0.046624	4.727814
222.868193	7710.343950	9.045837	-0.046647	4.730199
223.046704	7718.401253	9.050842	-0.046686	4.732598
223.068207	7726.368890	9.055847	-0.046695	4.734969
223.355714	7734.408207	9.060851	-0.046754	4.737360
223.291588	7742.394654	9.065856	-0.046748	4.739734
223.508067	7750.449925	9.070861	-0.046793	4.742127
223.667632	7758.410988	9.075866	-0.046828	4.744491
223.820324	7766.449655	9.080871	-0.046862	4.746877
223.807351	7774.469615	9.085875	-0.046865	4.749257
223.999421	7782.485300	9.090880	-0.046906	4.751633
224.407584	7790.558042	9.095885	-0.046988	4.754025
224.423647	7798.583163	9.100890	-0.046996	4.756402
224.468323	7806.479760	9.105895	-0.047010	4.758740
224.620214	7814.552448	9.110899	-0.047044	4.761129
224.756349	7822.493942	9.115904	-0.047074	4.763477
224.858283	7830.558355	9.120909	-0.047099	4.765861
225.084840	7838.586109	9.125914	-0.047146	4.768233
225.081152	7846.558001	9.130919	-0.047151	4.770588
225.142164	7854.629855	9.135923	-0.047168	4.772970
225.230808	7862.591830	9.140928	-0.047189	4.775319
225.550443	7870.643363	9.145933	-0.047254	4.777693
225.619001	7878.670289	9.150938	-0.047273	4.780058
225.624636	7886.650568	9.155943	-0.047279	4.782410
225.876579	7894.678429	9.160947	-0.047331	4.784773
225.913871	7902.686184	9.165952	-0.047344	4.787129
225.767287	7910.713382	9.170957	-0.047322	4.789492
226.036803	7918.750394	9.175962	-0.047377	4.791854
226.346015	7926.763366	9.180967	-0.047440	4.794207
226.276764	7934.806780	9.185971	-0.047433	4.796570
226.353542	7942.715904	9.190976	-0.047452	4.798892
226.641414	7950.777835	9.195981	-0.047511	4.801257
226.618302	7958.760365	9.200986	-0.047512	4.803598
226.580253	7966.804078	9.205991	-0.047511	4.805957
226.930360	7974.832191	9.210995	-0.047581	4.808308
226.997181	7982.823667	9.216000	-0.047599	4.810648
227.218321	7990.228426	9.221005	-0.047645	4.812814
227.286865	7994.674036	9.226010	-0.047661	4.814115

227.377676	7997.106308	9.231015	-0.047680	4.814826
227.449636	7998.502314	9.236019	-0.047694	4.815234
227.348672	7998.937210	9.241024	-0.047676	4.815362
227.583247	7999.816201	9.246029	-0.047720	4.815618
227.464207	7999.846312	9.251034	-0.047698	4.815627
227.600037	7999.895482	9.256039	-0.047724	4.815641
227.686972	7999.879822	9.261043	-0.047740	4.815636
227.716460	7999.809867	9.266048	-0.047746	4.815616
227.692246	7999.836173	9.271053	-0.047741	4.815623
227.834340	7999.824606	9.276058	-0.047768	4.815619
228.047675	7999.810987	9.281063	-0.047808	4.815614
228.150246	7999.923663	9.286067	-0.047827	4.815647
227.798960	7999.811267	9.291072	-0.047762	4.815616
228.046156	7999.876112	9.296077	-0.047808	4.815633
228.196461	7999.883890	9.301082	-0.047836	4.815635
228.297565	7999.794811	9.306087	-0.047855	4.815608
228.276314	7999.835041	9.311091	-0.047851	4.815620
228.323408	7999.825142	9.316096	-0.047860	4.815617
228.284927	7999.855487	9.321101	-0.047853	4.815626
228.238816	7999.850486	9.326106	-0.047845	4.815625
228.477161	7999.772163	9.331111	-0.047889	4.815601
228.476142	7999.825528	9.336115	-0.047889	4.815616
228.336799	7999.803011	9.341120	-0.047863	4.815611
228.508747	7999.869844	9.346125	-0.047896	4.815629
228.628840	7999.849383	9.351130	-0.047918	4.815623
228.388453	7999.826300	9.356135	-0.047873	4.815617
228.518239	7999.888182	9.361139	-0.047898	4.815635
228.662691	7999.884126	9.366144	-0.047925	4.815633
228.843077	7999.823012	9.371149	-0.047959	4.815614
228.592746	7999.871281	9.376154	-0.047912	4.815629
228.631067	7999.822815	9.381159	-0.047919	4.815615
228.633342	7999.863425	9.386163	-0.047920	4.815627
228.517445	7999.826343	9.391168	-0.047899	4.815616
228.732929	7999.865061	9.396173	-0.047939	4.815627
228.713557	7999.885042	9.401178	-0.047935	4.815633
228.582343	7999.830634	9.406183	-0.047911	4.815617
228.817960	7999.835522	9.411187	-0.047955	4.815618
228.758342	7999.797214	9.416192	-0.047944	4.815607
228.706591	7999.906330	9.421197	-0.047935	4.815639
228.897262	7999.826170	9.426202	-0.047970	4.815615
228.883466	7999.795006	9.431207	-0.047968	4.815606
229.153641	7999.874102	9.436211	-0.048018	4.815627
228.822039	7999.803647	9.441216	-0.047957	4.815608
229.114448	7999.885237	9.446221	-0.048011	4.815631
229.241210	7999.860614	9.451226	-0.048035	4.815623
229.048369	7999.800940	9.456231	-0.047999	4.815606
228.880409	7999.878293	9.461235	-0.047968	4.815630
228.939227	7999.789597	9.466240	-0.047979	4.815604
228.907214	7999.821115	9.471245	-0.047974	4.815613
228.899073	7999.858355	9.476250	-0.047972	4.815624
229.024955	7999.867874	9.481255	-0.047996	4.815626
229.149801	7999.851759	9.486259	-0.048019	4.815621
228.923298	7999.806485	9.491264	-0.047977	4.815609
229.052571	7999.850215	9.496269	-0.048002	4.815621
229.137196	7999.820642	9.501274	-0.048017	4.815612
229.158579	7999.791115	9.506279	-0.048022	4.815603
229.319666	7999.839629	9.511283	-0.048052	4.815616
229.223897	7999.793264	9.516288	-0.048034	4.815603
229.458597	7999.835497	9.521293	-0.048078	4.815615
229.337335	7999.901863	9.526298	-0.048055	4.815635
229.240244	7999.858679	9.531303	-0.048038	4.815622
229.245958	7999.897211	9.536307	-0.048039	4.815634
229.130234	7999.833446	9.541312	-0.048017	4.815616
229.224788	7999.833920	9.546317	-0.048035	4.815615
229.392930	7999.828112	9.551322	-0.048067	4.815613
229.343663	7999.811318	9.556327	-0.048058	4.815608
229.305726	7999.858751	9.561331	-0.048051	4.815622
229.486356	7999.877694	9.566336	-0.048084	4.815627
229.558015	7999.922629	9.571341	-0.048098	4.815640
229.477967	7999.912810	9.576346	-0.048083	4.815637
229.590346	7999.813237	9.581351	-0.048104	4.815607
229.365666	7999.898213	9.586355	-0.048063	4.815633
229.158728	7999.802019	9.591360	-0.048024	4.815606
229.389379	7999.840984	9.596365	-0.048067	4.815616
229.319205	7999.922052	9.601370	-0.048054	4.815641
229.382360	7999.866515	9.606375	-0.048066	4.815624
229.325340	7999.909369	9.611379	-0.048056	4.815637
229.421425	7999.861836	9.616384	-0.048074	4.815622
229.630130	7999.853482	9.621389	-0.048113	4.815619
229.485418	7999.898121	9.626394	-0.048086	4.815633
229.500768	7999.840744	9.631399	-0.048089	4.815616
229.710753	7999.915667	9.636403	-0.048128	4.815637
229.482876	7999.828740	9.641408	-0.048086	4.815612
229.613852	7999.820197	9.646413	-0.048111	4.815609
229.696420	7999.862106	9.651418	-0.048126	4.815621
229.624894	7999.857761	9.656423	-0.048113	4.815620
229.786984	7999.889214	9.661427	-0.048143	4.815629
229.643843	7999.836746	9.666432	-0.048117	4.815614
229.810028	7999.948321	9.671437	-0.048148	4.815646
229.850220	7999.911625	9.676442	-0.048156	4.815635
229.722348	7999.905301	9.681447	-0.048132	4.815634
229.894213	7999.920902	9.686451	-0.048164	4.815637
229.892386	7999.883527	9.691456	-0.048164	4.815626
229.821230	7999.878120	9.696461	-0.048151	4.815625
229.591640	7999.891501	9.701466	-0.048108	4.815630
229.832328	7999.869787	9.706471	-0.048153	4.815623
229.811628	7999.902556	9.711475	-0.048150	4.815632
229.799284	7999.830854	9.716480	-0.048147	4.815611
229.758509	7999.895319	9.721485	-0.048140	4.815631
229.817687	7999.905896	9.726490	-0.048151	4.815633
229.765894	7999.802602	9.731495	-0.048142	4.815603
229.726160	7999.839332	9.736499	-0.048134	4.815614
229.936557	7999.879038	9.741504	-0.048174	4.815625
229.904188	7999.862518	9.746509	-0.048168	4.815620
229.956326	7999.855902	9.751514	-0.048178	4.815618
230.052736	7999.820115	9.756519	-0.048196	4.815607
229.998164	7999.882223	9.761523	-0.048186	4.815626
229.817872	7999.830221	9.766528	-0.048152	4.815611
230.071393	7999.869558	9.771533	-0.048200	4.815621
230.047204	7999.851034	9.776538	-0.048195	4.815616
229.974039	7999.791158	9.781543	-0.048182	4.815599
230.129239	7999.852387	9.786547	-0.048211	4.815616
230.097686	7999.834812	9.791552	-0.048205	4.815611
230.065152	7999.850311	9.796557	-0.048199	4.815616
230.022301	7999.909406	9.801562	-0.048192	4.815633
230.070995	7999.846162	9.806567	-0.048201	4.815615
230.217151	7999.909381	9.811571	-0.048228	4.815632
230.124498	7999.840650	9.816576	-0.048211	4.815613
230.271589	7999.838772	9.821581	-0.048239	4.815611
230.139327	7999.888950	9.826586	-0.048214	4.815627
230.028715	7999.794311	9.831591	-0.048194	4.815600
230.086759	7999.844363	9.836595	-0.048205	4.815614
230.134335	7999.846213	9.841600	-0.048214	4.815614
230.187435	7999.841748	9.846605	-0.048224	4.815613
230.229510	7999.836037	9.851610	-0.048232	4.815611
230.175371	7999.819165	9.856615	-0.048222	4.815606
230.289648	7999.858385	9.861619	-0.048243	4.815617
230.047711	7999.836341	9.866624	-0.048198	4.815612
230.359116	7999.909704	9.871629	-0.048256	4.815632
230.317174	7999.881286	9.876634	-0.048249	4.815624
230.216135	7999.820958	9.881639	-0.048230	4.815606
230.207538	7999.868866	9.886643	-0.048229	4.815621
230.301878	7999.833046	9.891648	-0.048246	4.815610
230.429108	7999.839386	9.896653	-0.048270	4.815611
230.156009	7999.850995	9.901658	-0.048220	4.815616
230.152362	7999.816792	9.906663	-0.048219	4.815606
230.234406	7999.918469	9.911667	-0.048234	4.815635
230.264842	7999.877345	9.916672	-0.048240	4.815623
230.174462	7999.915391	9.921677	-0.048224	4.815634
230.251637	7999.948675	9.926682	-0.048238	4.815644
230.096059	7999.819151	9.931687	-0.048209	4.815606
230.155772	7999.878838	9.936691	-0.048221	4.815624
230.339344	7999.880752	9.941696	-0.048255	4.815623
230.390311	7999.916814	9.946701	-0.048265	4.815634
230.343444	7999.948092	9.951706	-0.048256	4.815643
230.354306	7999.870360	9.956711	-0.048258	4.815620
230.482797	7999.905541	9.961715	-0.048282	4.815630
230.259561	7999.899810	9.966720	-0.048241	4.815629
230.307953	7999.893134	9.971725	-0.048250	4.815627
230.453158	7999.921114	9.976730	-0.048277	4.815635
230.284089	7999.873562	9.981735	-0.048246	4.815621
230.394867	7999.916996	9.986739	-0.048267	4.815634
230.280427	7999.883136	9.991744	-0.048245	4.815624
230.490581	7999.902559	9.996749	-0.048285	4.815629
230.370078	7999.976411	10.001754	-0.048263	4.815651
230.379907	7999.842088	10.006759	-0.048264	4.815612
230.430403	7999.922975	10.011763	-0.048274	4.815635
230.265983	7999.917127	10.016768	-0.048244	4.815634
230.407078	7999.876725	10.021773	-0.048270	4.815622
230.417383	7999.868366	10.026778	-0.048272	4.815619
230.357092	7999.827910	10.031783	-0.048261	4.815608
230.453297	7999.880715	10.036787	-0.048279	4.815623
230.606626	7999.840512	10.041792	-0.048308	4.815610
230.718429	7999.897839	10.046797	-0.048329	4.815626
230.511005	7999.895565	10.051802	-0.048290	4.815627
230.538215	7999.840513	10.056807	-0.048295	4.815611
230.643436	7999.907341	10.061811	-0.048315	4.815630
230.446737	7999.872151	10.066816	-0.048279	4.815620
230.219037	7999.914381	10.071821	-0.048237	4.815634
230.369331	7999.880533	10.076826	-0.048265	4.815623
230.343619	7999.863052	10.081831	-0.048260	4.815618
230.150794	7999.918655	10.086835	-0.048224	4.815635
230.134641	7999.879980	10.091840	-0.048221	4.815624
230.359865	7999.919928	10.096845	-0.048264	4.815635
230.198009	7999.937605	10.101850	-0.048234	4.815641
230.257082	7999.933236	10.106855	-0.048245	4.815639
230.638305	7999.939415	10.111859	-0.048316	4.815639
230.348795	7999.924072	10.116864	-0.048262	4.815636
230.561403	7999.930726	10.121869	-0.048302	4.815637
230.552334	7999.911380	10.126874	-0.048300	4.815631
230.564043	7999.891301	10.131879	-0.048303	4.815625
230.590288	7999.939773	10.136883	-0.048308	4.815639
230.616453	7999.876165	10.141888	-0.048313	4.815621
230.671526	7999.974204	10.146893	-0.048323	4.815649
230.487742	7999.969110	10.151898	-0.048289	4.815648
230.549768	7999.922093	10.156903	-0.048301	4.815634
230.805130	8000.019103	10.161907	-0.048349	4.815661
230.721284	7999.941973	10.166912	-0.048333	4.815639
230.622393	7999.971342	10.171917	-0.048315	4.815648
230.739844	7999.979660	10.176922	-0.048337	4.815650
230.607492	7999.906015	10.181927	-0.048312	4.815629
230.566545	7999.914973	10.186931	-0.048305	4.815632
230.457030	7999.843833	10.191936	-0.048285	4.815612
230.528441	7999.862080	10.196941	-0.048298	4.815617
230.579921	7999.886409	10.201946	-0.048308	4.815624
230.619204	7999.884923	10.206951	-0.048315	4.815623
230.818366	7999.930855	10.211955	-0.048352	4.815636
230.632041	7999.858472	10.216960	-0.048318	4.815615
230.795677	7999.882481	10.221965	-0.048349	4.815621
230.745674	7999.896629	10.226970	-0.048339	4.815626
230.796648	7999.870782	10.231975	-0.048349	4.815618
230.849396	7999.914345	10.236979	-0.048359	4.815631
230.855817	7999.952890	10.241984	-0.048360	4.815642
230.662569	7999.934834	10.246989	-0.048325	4.815637
230.816898	7999.975771	10.251994	-0.048353	4.815649
230.636572	7999.896013	10.256999	-0.048320	4.815626
230.886729	7999.938500	10.262003	-0.048367	4.815637
230.803328	7999.906209	10.267008	-0.048351	4.815628
230.791804	7999.951935	10.272013	-0.048349	4.815642
230.612564	7999.936241	10.277018	-0.048316	4.815638
230.605287	7999.853945	10.282023	-0.048315	4.815614
230.636228	7999.877942	10.287027	-0.048321	4.815621
230.617440	7999.850966	10.292032	-0.048318	4.815613
230.813403	7999.868025	10.297037	-0.048354	4.815617
230.927796	7999.948879	10.302042	-0.048376	4.815640
230.697112	7999.862969	10.307047	-0.048333	4.815616
231.017772	7999.904461	10.312051	-0.048393	4.815627
230.928814	7999.917980	10.317056	-0.048376	4.815631
230.986045	7999.893301	10.322061	-0.048387	4.815624
231.005127	7999.959804	10.327066	-0.048391	4.815643
230.818230	7999.901288	10.332071	-0.048356	4.815627
230.947712	7999.930081	10.337075	-0.048380	4.815635
230.793603	7999.905186	10.342080	-0.048352	4.815628
230.933070	7999.933074	10.347085	-0.048378	4.815636
230.821860	7999.986795	10.352090	-0.048358	4.815652
230.680163	7999.910864	10.357095	-0.048331	4.815630
230.992971	7999.912734	10.362099	-0.048390	4.815629
230.875469	7999.900173	10.367104	-0.048368	4.815626
230.944841	7999.872488	10.372109	-0.048381	4.815618
230.928396	7999.894651	10.377114	-0.048378	4.815624
231.077466	7999.828760	10.382119	-0.048406	4.815604
231.198008	7999.971625	10.387123	-0.048429	4.815646
230.840716	7999.928499	10.392128	-0.048362	4.815635
231.111740	7999.922222	10.397133	-0.048413	4.815631
231.087645	7999.981622	10.402138	-0.048409	4.815649
230.988369	7999.956546	10.407143	-0.048390	4.815642
230.927079	7999.969444	10.412147	-0.048379	4.815646
230.852697	7999.935164	10.417152	-0.048365	4.815636
230.825084	7999.884562	10.422157	-0.048360	4.815622
230.875243	7999.956905	10.427162	-0.048370	4.815643
230.799760	7999.855359	10.432167	-0.048356	4.815613
230.757923	7999.856830	10.437171	-0.048348	4.815614
230.649459	7999.881775	10.442176	-0.048328	4.815622
230.687886	7999.922972	10.447181	-0.048335	4.815634
231.086979	7999.980678	10.452186	-0.048410	4.815649
230.920081	7999.911811	10.457191	-0.048379	4.815629
231.018015	7999.919813	10.462195	-0.048397	4.815631
231.143923	7999.906919	10.467200	-0.048421	4.815627
231.064227	7999.901374	10.472205	-0.048406	4.815626
230.848267	7999.920310	10.477210	-0.048366	4.815632
231.051175	7999.831806	10.482215	-0.048404	4.815605
231.125880	7999.941907	10.487219	-0.048418	4.815637
231.155377	7999.907172	10.492224	-0.048424	4.815627
231.019271	7999.880433	10.497229	-0.048399	4.815620
231.222150	7999.942437	10.502234	-0.048437	4.815637
230.970550	7999.859390	10.507239	-0.048390	4.815614
231.254883	7999.905633	10.512243	-0.048443	4.815626
231.044400	7999.818982	10.517248	-0.048404	4.815601
231.155755	7999.914731	10.522253	-0.048425	4.815629
231.003404	7999.926156	10.527258	-0.048397	4.815633
230.904323	7999.912825	10.532263	-0.048378	4.815630
230.925100	7999.914242	10.537267	-0.048382	4.815630
230.949356	7999.834591	10.542272	-0.048387	4.815606
230.844872	7999.942860	10.547277	-0.048368	4.815639
231.110582	7999.972790	10.552282	-0.048417	4.815646
231.000459	7999.872818	10.557287	-0.048397	4.815617
231.129924	8000.019030	10.562291	-0.048421	4.815660
231.173316	7999.936485	10.567296	-0.048430	4.815635
231.203849	7999.942329	10.572301	-0.048435	4.815637
231.016570	7999.955325	10.577306	-0.048401	4.815641
230.979249	7999.871475	10.582311	-0.048394	4.815617
231.304897	7999.894902	10.587315	-0.048455	4.815622
231.036180	7999.882029	10.592320	-0.048405	4.815620
231.173889	7999.903484	10.597325	-0.048431	4.815626
231.045886	7999.994294	10.602330	-0.048407	4.815653
230.914265	7999.966560	10.607335	-0.048383	4.815645
230.957455	7999.979014	10.612339	-0.048391	4.815649
230.985664	7999.945326	10.617344	-0.048396	4.815639
230.909815	7999.940910	10.622349	-0.048382	4.815638
230.968095	7999.961080	10.627354	-0.048393	4.815643
230.867950	7999.922113	10.632359	-0.048375	4.815632
231.022110	7999.973722	10.637363	-0.048404	4.815647
230.883733	7999.929867	10.642368	-0.048378	4.815635
230.947304	7999.920235	10.647373	-0.048390	4.815631
231.139233	8000.004479	10.652378	-0.048426	4.815655
231.066842	7999.917926	10.657383	-0.048413	4.815630
231.117595	7999.932637	10.662387	-0.048422	4.815634
231.058562	7999.959449	10.667392	-0.048411	4.815642
231.223660	7999.932245	10.672397	-0.048442	4.815634
231.203488	8000.053621	10.677402	-0.048439	4.815669
231.014612	8000.014285	10.682407	-0.048404	4.815659
231.092337	8000.032635	10.687411	-0.048418	4.815664
230.971530	7999.976254	10.692416	-0.048396	4.815648
230.988886	7999.884749	10.697421	-0.048399	4.815621
231.150625	7999.994123	10.702426	-0.048430	4.815652
231.221212	7999.925895	10.707431	-0.048443	4.815632
231.300775	7999.988040	10.712435	-0.048458	4.815650
231.269794	7999.941652	10.717440	-0.048452	4.815636
231.200001	7999.913850	10.722445	-0.048439	4.815628
231.328945	7999.999210	10.727450	-0.048464	4.815653
231.332296	7999.956580	10.732455	-0.048464	4.815640
231.448141	7999.922175	10.737459	-0.048486	4.815630
231.182257	7999.900808	10.742464	-0.048437	4.815625
231.287328	7999.935612	10.747469	-0.048456	4.815634
231.535853	7999.965265	10.752474	-0.048503	4.815642
231.422629	7999.980525	10.757479	-0.048482	4.815647
231.405244	8000.031495	10.762483	-0.048479	4.815662
231.330466	7999.968387	10.767488	-0.048465	4.815644
231.437565	7999.955189	10.772493	-0.048485	4.815639
231.357518	8000.005145	10.777498	-0.048470	4.815654
231.415676	7999.850252	10.782503	-0.048481	4.815609
231.461045	7999.943867	10.787507	-0.048490	4.815636
231.246230	7999.957484	10.792512	-0.048450	4.815641
231.120341	7999.960798	10.797517	-0.048427	4.815642
231.245535	7999.994860	10.802522	-0.048450	4.815652
231.142142	7999.940896	10.807527	-0.048431	4.815636
231.203517	7999.930161	10.812531	-0.048443	4.815633
231.151560	7999.948548	10.817536	-0.048433	4.815639
231.268853	7999.956863	10.822541	-0.048455	4.815641
231.266812	7999.980328	10.827546	-0.048455	4.815647
231.085705	7999.944320	10.832551	-0.048421	4.815638
231.432161	7999.951007	10.837555	-0.048486	4.815638
231.409117	7999.919691	10.842560	-0.048482	4.815629
231.266317	7999.949418	10.847565	-0.048456	4.815638
231.240655	7999.992781	10.852570	-0.048451	4.815651
231.244572	7999.938418	10.857575	-0.048452	4.815635
231.150648	7999.963598	10.862579	-0.048435	4.815643
231.276073	7999.953899	10.867584	-0.048458	4.815640
231.099288	7999.910490	10.872589	-0.048425	4.815628
231.140794	7999.977356	10.877594	-0.048433	4.815647
231.060009	7999.886398	10.882599	-0.048418	4.815621
231.096489	7999.952115	10.887603	-0.048425	4.815640
231.284694	7999.970118	10.892608	-0.048460	4.815644
231.353384	7999.912533	10.897613	-0.048473	4.815627
231.229629	7999.979928	10.902618	-0.048450	4.815647
231.288530	7999.912578	10.907623	-0.048462	4.815627
231.245169	7999.877732	10.912627	-0.048454	4.815617
231.252769	7999.931240	10.917632	-0.048455	4.815633
231.429974	7999.933053	10.922637	-0.048488	4.815633
231.244788	7999.917261	10.927642	-0.048454	4.815629
231.096868	7999.890331	10.932647	-0.048427	4.815622
231.139066	7999.931590	10.937651	-0.048435	4.815634
231.277740	7999.924239	10.942656	-0.048461	4.815631
231.308209	7999.880981	10.947661	-0.048466	4.815618
231.244677	7999.928001	10.952666	-0.048455	4.815632
231.310318	7999.925874	10.957671	-0.048467	4.815631
231.534461	7999.982887	10.962675	-0.048509	4.815647
231.346355	7999.940361	10.967680	-0.048474	4.815635
231.420127	7999.875387	10.972685	-0.048488	4.815616
231.431066	7999.940691	10.977690	-0.048490	4.815635
231.177082	7999.880021	10.982695	-0.048443	4.815618
231.341556	7999.963821	10.987699	-0.048474	4.815642
231.360020	7999.929975	10.992704	-0.048478	4.815632
231.371516	8000.000626	10.997709	-0.048480	4.815653
231.264029	8000.038396	11.002714	-0.048460	4.815664
231.266955	7999.990422	11.007719	-0.048461	4.815650
231.326360	7999.958305	11.012723	-0.048472	4.815641
231.366425	7999.980316	11.017728	-0.048480	4.815647
231.406775	7999.966038	11.022733	-0.048487	4.815642
231.334088	7999.948864	11.027738	-0.048474	4.815638
231.292067	7999.890555	11.032743	-0.048466	4.815621
231.299562	7999.891758	11.037747	-0.048468	4.815621
231.452098	7999.913453	11.042752	-0.048496	4.815627
231.401323	7999.893431	11.047757	-0.048487	4.815621
231.351448	7999.968426	11.052762	-0.048478	4.815643
231.294472	7999.968585	11.057767	-0.048467	4.815644
231.457584	8000.015003	11.062771	-0.048498	4.815656
231.396177	7999.963853	11.067776	-0.048487	4.815642
231.278346	7999.940611	11.072781	-0.048465	4.815636
231.539266	7999.939509	11.077786	-0.048514	4.815634
231.334790	7999.903123	11.082791	-0.048476	4.815624
231.361799	7999.995374	11.087795	-0.048481	4.815651
231.338399	7999.901073	11.092800	-0.048477	4.815624
231.575899	7999.914537	11.097805	-0.048521	4.815626
231.231945	8000.019999	11.102810	-0.048457	4.815659
231.446750	7999.938093	11.107815	-0.048497	4.815634
231.423700	8000.028467	11.112819	-0.048493	4.815660
231.196991	7999.937281	11.117824	-0.048451	4.815635
231.298989	7999.966698	11.122829	-0.048470	4.815643
231.461726	7999.940524	11.127834	-0.048501	4.815635
231.436442	7999.965747	11.132839	-0.048496	4.815642
231.301763	7999.995605	11.137843	-0.048471	4.815651
231.377504	7999.981899	11.142848	-0.048485	4.815647
231.563089	7999.969972	11.147853	-0.048520	4.815643
231.445980	7999.964888	11.152858	-0.048499	4.815642
231.278734	7999.883204	11.157863	-0.048467	4.815619
231.426266	7999.882402	11.162867	-0.048495	4.815618
231.370750	7999.929552	11.167872	-0.048485	4.815632
231.353343	7999.867372	11.172877	-0.048482	4.815614
231.536275	7999.902369	11.177882	-0.048516	4.815623
231.484587	7999.903681	11.182887	-0.048507	4.815624
231.476828	7999.959076	11.187891	-0.048505	4.815640
231.599376	8000.000569	11.192896	-0.048528	4.815651
231.593784	7999.975940	11.197901	-0.048527	4.815644
231.502382	7999.961665	11.202906	-0.048511	4.815641
231.321333	7999.833858	11.207911	-0.048477	4.815604
231.478937	7999.904738	11.212915	-0.048506	4.815624
231.420846	7999.894204	11.217920	-0.048496	4.815621
231.419149	7999.864302	11.222925	-0.048496	4.815612
231.655354	7999.963140	11.227930	-0.048540	4.815640
231.582080	7999.874437	11.232935	-0.048526	4.815615
231.504473	7999.945781	11.237939	-0.048512	4.815636
231.701618	7999.916961	11.242944	-0.048549	4.815626
231.710962	7999.906451	11.247949	-0.048551	4.815623
231.639754	7999.998181	11.252954	-0.048538	4.815651
231.446094	7999.940621	11.257959	-0.048502	4.815635
231.793853	8000.061548	11.262963	-0.048567	4.815668
231.727903	7999.968692	11.267968	-0.048555	4.815641
231.535228	7999.959183	11.272973	-0.048519	4.815640
231.681981	7999.903928	11.277978	-0.048546	4.815623
231.896873	7999.902082	11.282983	-0.048586	4.815621
231.857210	7999.993255	11.287987	-0.048579	4.815648
231.566165	7999.944793	11.292992	-0.048525	4.815635
231.645615	7999.904461	11.297997	-0.048540	4.815623
231.501846	7999.964061	11.303002	-0.048514	4.815641
231.442228	7999.933221	11.308007	-0.048503	4.815632
231.670162	7999.955069	11.313011	-0.048545	4.815638
231.573951	7999.959930	11.318016	-0.048527	4.815640
231.497249	7999.907465	11.323021	-0.048513	4.815625
231.644299	7999.932274	11.328026	-0.048541	4.815631
231.747143	7999.974516	11.333031	-0.048560	4.815643
231.904012	8000.008024	11.338035	-0.048590	4.815652
231.691865	7999.970446	11.343040	-0.048550	4.815642
231.769463	7999.935421	11.348045	-0.048565	4.815631
231.954868	7999.952312	11.353050	-0.048599	4.815636
231.750205	7999.887101	11.358055	-0.048561	4.815617
231.660327	7999.901672	11.363059	-0.048545	4.815622
231.620510	7999.909581	11.368064	-0.048538	4.815625
231.566064	7999.868150	11.373069	-0.048528	4.815613
231.591972	7999.893134	11.378074	-0.048533	4.815620
231.601151	7999.892229	11.383079	-0.048534	4.815620
231.578886	7999.937782	11.388083	-0.048531	4.815633
231.690439	7999.954545	11.393088	-0.048551	4.815637
231.559569	7999.921485	11.398093	-0.048527	4.815628
231.654981	7999.924110	11.403098	-0.048545	4.815629
231.521548	7999.860052	11.408103	-0.048520	4.815611
231.843817	7999.935732	11.413107	-0.048581	4.815631
231.957005	7999.994153	11.418112	-0.048602	4.815648
231.895774	7999.892834	11.423117	-0.048591	4.815618
231.936019	7999.983166	11.428122	-0.048598	4.815645
231.862554	7999.948899	11.433127	-0.048585	4.815635
231.783760	7999.955109	11.438131	-0.048570	4.815637
231.866171	7999.937242	11.443136	-0.048586	4.815631
231.842038	7999.910178	11.448141	-0.048581	4.815624
231.973942	7999.965700	11.453146	-0.048606	4.815639
231.848918	7999.916721	11.458151	-0.048583	4.815626
231.740433	7999.940598	11.463155	-0.048563	4.815633
231.813408	7999.968479	11.468160	-0.048577	4.815641
231.854173	7999.955276	11.473165	-0.048584	4.815637
231.764010	7999.998663	11.478170	-0.048568	4.815650
231.867520	7999.962991	11.483175	-0.048587	4.815639
231.863485	8000.002435	11.488179	-0.048587	4.815651
231.782520	7999.925348	11.493184	-0.048572	4.815628
231.842630	7999.924200	11.498189	-0.048583	4.815628
231.963097	7999.946445	11.503194	-0.048606	4.815634
231.782363	7999.930724	11.508199	-0.048572	4.815630
231.780199	7999.974468	11.513203	-0.048572	4.815643
231.714002	7999.899755	11.518208	-0.048560	4.815621
231.717096	7999.885942	11.523213	-0.048560	4.815617
231.667156	7999.964139	11.528218	-0.048551	4.815640
231.669236	7999.903341	11.533223	-0.048552	4.815622
231.922618	7999.907455	11.538227	-0.048599	4.815622
231.671330	7999.989866	11.543232	-0.048553	4.815648
231.755315	7999.963485	11.548237	-0.048568	4.815640
231.859615	8000.016425	11.553242	-0.048588	4.815655
231.593518	7999.973703	11.558247	-0.048539	4.815643
231.761835	7999.925202	11.563251	-0.048570	4.815628
231.676608	7999.972939	11.568256	-0.048554	4.815643
231.794028	7999.915075	11.573261	-0.048576	4.815625
231.737083	7999.951528	11.578266	-0.048566	4.815636
231.594642	7999.923618	11.583271	-0.048539	4.815629
231.808823	7999.975133	11.588275	-0.048580	4.815643
231.817444	7999.968881	11.593280	-0.048581	4.815641
231.701424	7999.937128	11.598285	-0.048560	4.815632
231.970689	7999.961781	11.603290	-0.048610	4.815638
231.776958	7999.879667	11.608295	-0.048574	4.815615
232.024974	7999.927460	11.613299	-0.048621	4.815628
231.891152	7999.966939	11.618304	-0.048596	4.815640
231.787565	7999.886284	11.623309	-0.048577	4.815617
231.772819	7999.946904	11.628314	-0.048574	4.815635
231.809216	7999.894134	11.633319	-0.048581	4.815619
231.839933	7999.967231	11.638323	-0.048587	4.815640
231.774488	7999.976860	11.643328	-0.048575	4.815643
231.876483	7999.969985	11.648333	-0.048594	4.815641
232.165845	8000.001369	11.653338	-0.048648	4.815649
232.083967	7999.982977	11.658343	-0.048633	4.815644
231.935946	7999.984865	11.663347	-0.048606	4.815645
231.818317	7999.926399	11.668352	-0.048584	4.815628
231.965729	7999.907449	11.673357	-0.048611	4.815622
231.952877	7999.973437	11.678362	-0.048609	4.815641
232.040534	7999.856381	11.683367	-0.048626	4.815607
232.113794	7999.900278	11.688371	-0.048639	4.815619
231.919633	7999.925971	11.693376	-0.048603	4.815628
232.011908	7999.881577	11.698381	-0.048621	4.815614
232.101018	7999.940676	11.703386	-0.048637	4.815631
232.003688	7999.928439	11.708391	-0.048620	4.815628
231.967199	7999.951346	11.713395	-0.048613	4.815635
231.959151	7999.932015	11.718400	-0.048612	4.815629
232.156704	7999.921349	11.723405	-0.048648	4.815625
231.962120	7999.933158	11.728410	-0.048612	4.815630
232.103609	7999.952541	11.733415	-0.048639	4.815635
232.110306	7999.979349	11.738419	-0.048640	4.815642
232.109527	7999.949461	11.743424	-0.048640	4.815634
232.191491	7999.856864	11.748429	-0.048656	4.815606
232.209959	7999.948978	11.753434	-0.048659	4.815633
232.019900	7999.888273	11.758439	-0.048624	4.815616
232.075466	7999.942559	11.763443	-0.048635	4.815632
231.957763	7999.957746	11.768448	-0.048613	4.815637
232.218528	7999.895798	11.773453	-0.048662	4.815617
232.112442	7999.982694	11.778458	-0.048642	4.815643
232.209413	7999.936241	11.783463	-0.048660	4.815629
232.012891	7999.992852	11.788467	-0.048624	4.815647
232.123377	7999.992519	11.793472	-0.048644	4.815646
232.069115	7999.936145	11.798477	-0.048634	4.815630
232.074443	8000.002428	11.803482	-0.048636	4.815649
232.070000	7999.986358	11.808487	-0.048635	4.815645
232.023615	7999.969608	11.813491	-0.048627	4.815640
232.001070	7999.990606	11.818496	-0.048622	4.815646
232.183642	7999.948741	11.823501	-0.048657	4.815633
232.179075	8000.012729	11.828506	-0.048656	4.815652
231.907719	7999.975259	11.833511	-0.048606	4.815642
232.192976	8000.011913	11.838515	-0.048659	4.815651
232.040048	7999.948606	11.843520	-0.048630	4.815634
232.022634	7999.925920	11.848525	-0.048627	4.815627
232.266503	7999.960838	11.853530	-0.048673	4.815636
232.015719	7999.921566	11.858535	-0.048626	4.815626
232.100188	7999.989129	11.863539	-0.048642	4.815645
232.005414	7999.957720	11.868544	-0.048625	4.815636
232.213491	7999.934414	11.873549	-0.048664	4.815629
232.068168	7999.973707	11.878554	-0.048637	4.815641
231.959873	7999.943146	11.883559	-0.048617	4.815632
232.299956	8000.004173	11.888563	-0.048680	4.815649
232.122321	7999.956477	11.893568	-0.048647	4.815636
232.065099	7999.967306	11.898573	-0.048637	4.815639
231.943133	7999.965346	11.903578	-0.048614	4.815639
232.108497	7999.907190	11.908583	-0.048645	4.815621
231.918442	7999.950028	11.913587	-0.048610	4.815635
231.925970	7999.941624	11.918592	-0.048612	4.815632
231.981465	7999.889162	11.923597	-0.048622	4.815616
232.134805	7999.942896	11.928602	-0.048651	4.815631
232.153179	7999.897306	11.933607	-0.048654	4.815618
232.078667	7999.922800	11.938611	-0.048641	4.815626
232.084840	7999.897294	11.943616	-0.048642	4.815618
232.133625	7999.890625	11.948621	-0.048651	4.815616
232.092802	7999.916664	11.953626	-0.048644	4.815624
232.145438	7999.872696	11.958631	-0.048654	4.815611
232.158277	7999.911346	11.963635	-0.048656	4.815622
232.168504	7999.917930	11.968640	-0.048658	4.815624
232.271542	7999.904666	11.973645	-0.048678	4.815620
232.167891	7999.894463	11.978650	-0.048658	4.815617
232.127188	7999.893817	11.983655	-0.048651	4.815617
232.331556	7999.956917	11.988659	-0.048689	4.815635
232.201630	7999.916398	11.993664	-0.048665	4.815623
232.078477	7999.909081	11.998669	-0.048642	4.815622
232.213742	8000.022301	12.003674	-0.048668	4.815654
232.249821	7999.910814	12.008679	-0.048675	4.815621
232.098930	7999.916925	12.013683	-0.048647	4.815624
232.213944	7999.925205	12.018688	-0.048668	4.815626
232.331555	7999.887626	12.023693	-0.048690	4.815614
232.190881	7999.953680	12.028698	-0.048664	4.815634
232.110388	7999.921434	12.033703	-0.048649	4.815625
232.216102	7999.914619	12.038707	-0.048669	4.815623
232.112066	7999.917218	12.043712	-0.048650	4.815624
231.970235	7999.894654	12.048717	-0.048624	4.815618
232.021273	7999.977689	12.053722	-0.048634	4.815642
232.141250	7999.997792	12.058727	-0.048656	4.815647
232.187576	7999.997487	12.063731	-0.048665	4.815647
232.081747	8000.003260	12.068736	-0.048645	4.815649
232.109028	7999.957814	12.073741	-0.048650	4.815636
232.199571	7999.981710	12.078746	-0.048667	4.815642
232.246597	7999.961135	12.083751	-0.048676	4.815636
232.159835	7999.945867	12.088755	-0.048660	4.815632
232.230813	7999.960906	12.093760	-0.048674	4.815636
232.159466	7999.972575	12.098765	-0.048661	4.815640
232.308982	7999.973941	12.103770	-0.048689	4.815640
232.325649	7999.892029	12.108775	-0.048692	4.815616
232.221351	7999.931985	12.113779	-0.048673	4.815628
231.967693	7999.950310	12.118784	-0.048626	4.815634
232.046896	7999.980427	12.123789	-0.048640	4.815643
232.209016	7999.951041	12.128794	-0.048671	4.815633
231.922410	7999.981642	12.133799	-0.048618	4.815644
232.048461	7999.987965	12.138803	-0.048641	4.815645
232.266418	7999.993642	12.143808	-0.048682	4.815646
232.067777	7999.952011	12.148813	-0.048645	4.815634
232.101940	7999.998479	12.153818	-0.048652	4.815648
231.982193	7999.946383	12.158823	-0.048629	4.815633
232.200344	7999.941387	12.163827	-0.048670	4.815631
232.050142	7999.937902	12.168832	-0.048642	4.815630
232.180563	7999.885586	12.173837	-0.048667	4.815614
232.147004	7999.932025	12.178842	-0.048661	4.815628
231.962899	7999.899169	12.183847	-0.048627	4.815619
232.192779	7999.941332	12.188851	-0.048670	4.815631
232.247402	7999.950770	12.193856	-0.048680	4.815633
232.185917	7999.914561	12.198861	-0.048669	4.815623
232.261018	7999.956354	12.203866	-0.048683	4.815635
232.275044	7999.910693	12.208871	-0.048686	4.815621
232.414615	7999.908696	12.213875	-0.048712	4.815620
232.216753	7999.914047	12.218880	-0.048675	4.815622
232.189956	7999.839971	12.223885	-0.048670	4.815601
232.339487	7999.904318	12.228890	-0.048698	4.815619
232.340455	7999.876593	12.233895	-0.048698	4.815611
232.191634	7999.964933	12.238899	-0.048671	4.815637
232.425492	7999.963395	12.243904	-0.048715	4.815636
232.428260	8000.005085	12.248909	-0.048715	4.815648
232.096435	7999.968770	12.253914	-0.048654	4.815639
232.314379	7999.858091	12.258919	-0.048694	4.815606
232.534084	7999.888348	12.263923	-0.048735	4.815613
232.370196	7999.947622	12.268928	-0.048705	4.815631
232.527749	7999.890407	12.273933	-0.048735	4.815614
232.398464	7999.988671	12.278938	-0.048711	4.815643
232.446612	7999.939292	12.283943	-0.048720	4.815629
232.446783	7999.914756	12.288947	-0.048720	4.815621
232.478633	7999.925960	12.293952	-0.048726	4.815625
232.270670	7999.890583	12.298957	-0.048687	4.815615
232.343134	7999.975033	12.303962	-0.048701	4.815640
232.429305	7999.923067	12.308967	-0.048717	4.815624
232.298222	7999.913486	12.313971	-0.048693	4.815622
232.217411	7999.882303	12.318976	-0.048678	4.815613
232.181494	7999.891342	12.323981	-0.048672	4.815616
232.319768	7999.983262	12.328986	-0.048698	4.815642
232.278716	7999.954856	12.333991	-0.048690	4.815634
232.282787	7999.961340	12.338995	-0.048691	4.815636
232.252472	7999.941648	12.344000	-0.048686	4.815630
232.248654	7999.904239	12.349005	-0.048685	4.815619
232.237886	7999.988408	12.354010	-0.048683	4.815644
232.232144	7999.909336	12.359015	-0.048682	4.815621
232.414993	7999.900567	12.364019	-0.048716	4.815617
232.399195	7999.880042	12.369024	-0.048714	4.815611
232.392420	7999.871406	12.374029	-0.048712	4.815609
232.353146	7999.978599	12.379034	-0.048705	4.815641
232.251100	7999.861674	12.384039	-0.048686	4.815607
232.165653	7999.882721	12.389043	-0.048671	4.815613
232.320426	7999.878835	12.394048	-0.048700	4.815611
232.229724	7999.844288	12.399053	-0.048683	4.815602
232.120355	7999.918322	12.404058	-0.048663	4.815624
232.174742	7999.845560	12.409063	-0.048673	4.815602
232.316073	7999.857469	12.414067	-0.048699	4.815605
232.229143	7999.867817	12.419072	-0.048683	4.815609
232.355980	7999.881626	12.424077	-0.048707	4.815612
232.547089	7999.938107	12.429082	-0.048743	4.815628
232.465139	7999.857800	12.434087	-0.048728	4.815605
232.344371	7999.902828	12.439091	-0.048706	4.815618
232.464344	7999.909053	12.444096	-0.048728	4.815620
232.299868	7999.904269	12.449101	-0.048698	4.815619
232.320233	7999.955851	12.454106	-0.048702	4.815634
232.251319	7999.916320	12.459111	-0.048689	4.815623
232.341361	7999.956220	12.464115	-0.048706	4.815634
232.448426	7999.967574	12.469120	-0.048726	4.815637
232.325471	7999.911156	12.474125	-0.048703	4.815621
232.516232	7999.924932	12.479130	-0.048739	4.815624
232.496908	7999.856314	12.484135	-0.048735	4.815604
232.513595	7999.896095	12.489139	-0.048739	4.815616
232.464786	7999.943354	12.494144	-0.048730	4.815630
232.492643	7999.890445	12.499149	-0.048735	4.815614
232.496018	7999.960967	12.504154	-0.048736	4.815635
232.341590	7999.967020	12.509159	-0.048707	4.815637
232.554662	7999.930986	12.514163	-0.048747	4.815626
232.454238	7999.972073	12.519168	-0.048729	4.815638
232.266116	7999.881508	12.524173	-0.048694	4.815612
232.453910	7999.942205	12.529178	-0.048729	4.815629
232.404127	7999.930738	12.534183	-0.048720	4.815626
232.457676	7999.940158	12.539187	-0.048730	4.815629
232.449501	7999.927230	12.544192	-0.048728	4.815625
232.567696	7999.887525	12.549197	-0.048751	4.815613
232.747234	7999.993991	12.554202	-0.048784	4.815643
232.513336	7999.958193	12.559207	-0.048741	4.815634
232.760371	7999.956868	12.564211	-0.048787	4.815632
232.660189	7999.913628	12.569216	-0.048768	4.815620
232.630668	7999.891814	12.574221	-0.048763	4.815614
232.489039	7999.961056	12.579226	-0.048737	4.815635
232.470345	7999.929810	12.584231	-0.048734	4.815626
232.463765	7999.955336	12.589235	-0.048732	4.815633
232.390745	7999.898659	12.594240	-0.048719	4.815617
232.362485	7999.875798	12.599245	-0.048714	4.815610
232.530013	7999.947909	12.604250	-0.048745	4.815631
232.455489	7999.946716	12.609255	-0.048732	4.815631
232.482550	7999.956775	12.614259	-0.048737	4.815633
232.696449	7999.938902	12.619264	-0.048777	4.815627
232.691066	7999.876914	12.624269	-0.048776	4.815609
232.567922	7999.987020	12.629274	-0.048753	4.815642
232.536170	7999.958765	12.634279	-0.048747	4.815634
232.706314	7999.994625	12.639283	-0.048779	4.815643
232.553944	7999.966552	12.644288	-0.048751	4.815636
232.506051	7999.924158	12.649293	-0.048742	4.815624
232.804784	7999.980247	12.654298	-0.048798	4.815639
232.597622	7999.910723	12.659303	-0.048760	4.815619
232.635905	7999.940178	12.664307	-0.048767	4.815628
232.669642	7999.951412	12.669312	-0.048773	4.815631
232.538136	7999.920475	12.674317	-0.048749	4.815622
232.551309	8000.028518	12.679322	-0.048752	4.815654
232.413770	7999.962255	12.684327	-0.048726	4.815635
232.504601	7999.986156	12.689331	-0.048743	4.815642
232.451244	7999.918054	12.694336	-0.048733	4.815622
232.361699	7999.957183	12.699341	-0.048717	4.815634
232.635571	8000.027814	12.704346	-0.048768	4.815653
232.435800	7999.919980	12.709351	-0.048731	4.815623
232.507054	7999.968116	12.714355	-0.048744	4.815636
232.576797	8000.014093	12.719360	-0.048758	4.815650
232.565359	7999.953075	12.724365	-0.048756	4.815632
232.638668	7999.990570	12.729370	-0.048769	4.815642
232.826887	7999.951999	12.734375	-0.048805	4.815630
232.862880	7999.947257	12.739379	-0.048811	4.815629
232.509555	7999.945820	12.744384	-0.048746	4.815630
232.635863	7999.871020	12.749389	-0.048769	4.815607
232.751372	7999.955100	12.754394	-0.048791	4.815631
232.543618	7999.882363	12.759399	-0.048753	4.815611
232.697269	7999.862447	12.764403	-0.048781	4.815605
232.758996	7999.983018	12.769408	-0.048793	4.815640
232.666553	7999.996480	12.774413	-0.048776	4.815644
232.552682	8000.017067	12.779418	-0.048755	4.815651
232.518688	7999.970628	12.784423	-0.048749	4.815637
232.765944	7999.921270	12.789427	-0.048795	4.815621
232.632773	7999.969300	12.794432	-0.048770	4.815636
232.440128	7999.928832	12.799437	-0.048735	4.815625
232.710927	7999.979132	12.804442	-0.048785	4.815639
232.546009	7999.898549	12.809447	-0.048755	4.815616
232.677247	7999.890012	12.814451	-0.048779	4.815613
232.692369	7999.950050	12.819456	-0.048782	4.815630
232.905355	7999.871315	12.824461	-0.048822	4.815606
232.661151	7999.958111	12.829466	-0.048777	4.815633
232.502517	7999.901114	12.834471	-0.048747	4.815617
232.664188	7999.910150	12.839475	-0.048778	4.815619
232.597684	7999.960326	12.844480	-0.048765	4.815634
232.549477	7999.910455	12.849485	-0.048756	4.815619
232.799862	7999.955087	12.854490	-0.048803	4.815631
232.760644	7999.904293	12.859495	-0.048796	4.815616
232.587923	7999.904713	12.864499	-0.048764	4.815617
232.749785	7999.926562	12.869504	-0.048794	4.815623
232.853987	7999.865280	12.874509	-0.048814	4.815605
232.783524	7999.968767	12.879514	-0.048801	4.815635
232.695366	7999.873414	12.884519	-0.048785	4.815608
232.770389	7999.892789	12.889523	-0.048799	4.815613
232.744700	7999.906264	12.894528	-0.048794	4.815617
232.563795	7999.849975	12.899533	-0.048761	4.815601
232.817986	7999.959785	12.904538	-0.048808	4.815632
232.875876	7999.963938	12.909543	-0.048819	4.815633
232.785776	7999.914456	12.914547	-0.048802	4.815619
232.816725	7999.951265	12.919552	-0.048808	4.815630
232.891654	7999.877767	12.924557	-0.048822	4.815608
232.720453	7999.945463	12.929562	-0.048791	4.815629
232.685138	7999.954512	12.934567	-0.048784	4.815631
232.867902	7999.977767	12.939571	-0.048819	4.815637
232.839354	8000.014681	12.944576	-0.048813	4.815648
232.707926	7999.938909	12.949581	-0.048789	4.815627
233.033975	7999.937797	12.954586	-0.048850	4.815625
232.914856	7999.855820	12.959591	-0.048828	4.815601
232.769358	7999.892975	12.964595	-0.048801	4.815613
232.812537	7999.908632	12.969600	-0.048809	4.815617
232.982122	7999.879367	12.974605	-0.048841	4.815608
232.723664	7999.974472	12.979610	-0.048793	4.815637
232.647384	7999.838747	12.984615	-0.048779	4.815598
232.799366	7999.876448	12.989619	-0.048807	4.815608
232.910144	7999.942305	12.994624	-0.048828	4.815627
232.830995	7999.878055	12.999629	-0.048813	4.815608
232.866561	7999.875442	13.004634	-0.048820	4.815607
233.025751	7999.852413	13.009639	-0.048850	4.815600
232.912430	7999.895426	13.014643	-0.048829	4.815613
232.914854	7999.893344	13.019648	-0.048830	4.815612
232.980281	7999.862392	13.024653	-0.048842	4.815603
233.240100	7999.898637	13.029658	-0.048891	4.815612
232.804569	7999.858506	13.034663	-0.048810	4.815603
232.774618	7999.937029	13.039667	-0.048804	4.815626
232.941494	7999.940812	13.044672	-0.048836	4.815626
232.803061	7999.875602	13.049677	-0.048810	4.815608
232.978354	7999.914749	13.054682	-0.048843	4.815618
232.958496	7999.916575	13.059687	-0.048839	4.815619
233.037482	7999.851683	13.064691	-0.048854	4.815600
233.027511	7999.820578	13.069696	-0.048852	4.815591
232.986931	7999.814597	13.074701	-0.048845	4.815589
232.995242	7999.896942	13.079706	-0.048847	4.815613
232.771587	7999.898672	13.084711	-0.048805	4.815615
232.961221	7999.904958	13.089715	-0.048841	4.815616
233.069638	7999.949427	13.094720	-0.048861	4.815628
232.949991	7999.883453	13.099725	-0.048839	4.815609
233.084889	7999.921946	13.104730	-0.048864	4.815620
233.281765	7999.925148	13.109735	-0.048901	4.815620
233.211758	7999.913352	13.114739	-0.048888	4.815617
232.890947	7999.896429	13.119744	-0.048828	4.815613
233.084765	7999.889973	13.124749	-0.048865	4.815611
233.157194	7999.931724	13.129754	-0.048878	4.815622
233.011430	7999.925107	13.134759	-0.048851	4.815621
233.061978	7999.901387	13.139763	-0.048861	4.815614
232.908699	7999.901053	13.144768	-0.048832	4.815615
233.095211	7999.870994	13.149773	-0.048867	4.815605
233.098358	7999.954324	13.154778	-0.048868	4.815629
233.022985	7999.896539	13.159783	-0.048854	4.815613
233.033619	7999.854025	13.164787	-0.048856	4.815600
233.041807	7999.949178	13.169792	-0.048858	4.815628
232.942411	7999.935840	13.174797	-0.048840	4.815625
233.185004	7999.968604	13.179802	-0.048885	4.815633
233.082794	7999.950950	13.184807	-0.048866	4.815628
232.981680	7999.934381	13.189811	-0.048847	4.815624
233.180203	7999.946149	13.194816	-0.048885	4.815626
233.035157	7999.876562	13.199821	-0.048858	4.815607
232.891814	7999.851837	13.204826	-0.048831	4.815600
232.994923	7999.848182	13.209831	-0.048851	4.815599
233.027739	7999.830580	13.214835	-0.048857	4.815593
232.938741	7999.930564	13.219840	-0.048840	4.815623
232.988820	7999.905769	13.224845	-0.048850	4.815616
232.971567	7999.941798	13.229850	-0.048847	4.815626
232.942752	7999.867687	13.234855	-0.048842	4.815605
233.028744	7999.881903	13.239859	-0.048858	4.815608
233.051250	7999.890821	13.244864	-0.048862	4.815611
232.835106	7999.864917	13.249869	-0.048822	4.815604
232.872312	7999.887951	13.254874	-0.048829	4.815611
232.902684	7999.842554	13.259879	-0.048835	4.815597
233.029364	7999.923613	13.264883	-0.048859	4.815621
233.087561	7999.929906	13.269888	-0.048870	4.815622
232.977039	7999.861945	13.274893	-0.048849	4.815603
232.973385	7999.919544	13.279898	-0.048849	4.815620
232.880228	7999.897767	13.284903	-0.048832	4.815614
232.990107	7999.876075	13.289907	-0.048852	4.815607
233.079681	7999.922373	13.294912	-0.048869	4.815620
232.867815	7999.909349	13.299917	-0.048830	4.815617
232.932969	7999.933902	13.304922	-0.048842	4.815624
232.888134	7999.931055	13.309927	-0.048834	4.815623
233.128829	7999.914683	13.314931	-0.048879	4.815617
232.862968	7999.954159	13.319936	-0.048829	4.815630
232.801999	7999.897676	13.324941	-0.048818	4.815614
233.063304	7999.951025	13.329946	-0.048867	4.815628
232.977979	7999.854650	13.334951	-0.048851	4.815601
232.913163	7999.864289	13.339955	-0.048839	4.815604
233.030139	7999.888614	13.344960	-0.048861	4.815610
233.019823	7999.866043	13.349965	-0.048859	4.815604
233.132020	7999.886020	13.354970	-0.048881	4.815609
232.962008	7999.898226	13.359975	-0.048849	4.815613
233.019996	7999.911988	13.364979	-0.048860	4.815617
232.966759	7999.921815	13.369984	-0.048850	4.815620
232.946257	7999.920429	13.374989	-0.048847	4.815620
233.182784	7999.934947	13.379994	-0.048891	4.815623
233.178123	7999.921008	13.384999	-0.048890	4.815619
233.050057	7999.880517	13.390003	-0.048866	4.815608
233.133822	7999.939532	13.395008	-0.048882	4.815625
233.232179	7999.886696	13.400013	-0.048901	4.815609
233.212672	7999.930161	13.405018	-0.048897	4.815621
233.070130	7999.908651	13.410023	-0.048871	4.815616
233.045500	7999.881578	13.415027	-0.048866	4.815608
233.114236	7999.908325	13.420032	-0.048879	4.815616
233.008669	7999.951464	13.425037	-0.048860	4.815629
233.280681	7999.977233	13.430042	-0.048911	4.815635
233.106505	7999.944535	13.435047	-0.048878	4.815626
232.841163	7999.910362	13.440051	-0.048829	4.815617
233.037754	7999.949854	13.445056	-0.048866	4.815628
233.028962	7999.896350	13.450061	-0.048864	4.815612
232.940823	7999.907746	13.455066	-0.048848	4.815616
232.848082	7999.946823	13.460071	-0.048831	4.815628
233.098534	7999.964769	13.465075	-0.048878	4.815632
233.027082	7999.901711	13.470080	-0.048865	4.815614
232.793357	7999.869118	13.475085	-0.048821	4.815606
233.028225	7999.863326	13.480090	-0.048865	4.815603
232.892644	7999.888899	13.485095	-0.048840	4.815611
232.990073	7999.884086	13.490099	-0.048858	4.815609
232.932723	7999.946153	13.495104	-0.048848	4.815627
232.877937	7999.904714	13.500109	-0.048838	4.815616
233.050532	7999.958762	13.505114	-0.048870	4.815631
232.968404	7999.944636	13.510119	-0.048855	4.815627
232.936925	7999.898237	13.515123	-0.048849	4.815613
232.981335	7999.936332	13.520128	-0.048858	4.815624
232.846143	7999.918144	13.525133	-0.048833	4.815620
233.070338	7999.900438	13.530138	-0.048875	4.815613
232.987622	7999.882032	13.535143	-0.048859	4.815608
233.038155	7999.862581	13.540147	-0.048869	4.815602
233.081907	7999.976458	13.545152	-0.048877	4.815636
233.334956	7999.941072	13.550157	-0.048924	4.815624
233.308691	7999.969483	13.555162	-0.048920	4.815632
233.105454	7999.960867	13.560167	-0.048882	4.815631
233.130606	7999.954883	13.565171	-0.048887	4.815629
233.299309	7999.945886	13.570176	-0.048918	4.815626
233.112067	7999.978095	13.575181	-0.048884	4.815636
233.211914	7999.941295	13.580186	-0.048902	4.815625
233.108970	7999.923629	13.585191	-0.048883	4.815620
233.067608	7999.931513	13.590195	-0.048876	4.815622
233.152290	7999.938235	13.595200	-0.048892	4.815624
233.093005	7999.872171	13.600205	-0.048881	4.815605
232.979983	7999.956822	13.605210	-0.048860	4.815630
232.980408	7999.874645	13.610215	-0.048860	4.815606
233.187969	7999.886559	13.615219	-0.048899	4.815609
233.204277	7999.966900	13.620224	-0.048902	4.815632
233.070245	7999.901760	13.625229	-0.048877	4.815614
233.330480	7999.954025	13.630234	-0.048926	4.815628
233.159960	7999.984370	13.635239	-0.048894	4.815637
232.968318	7999.956727	13.640243	-0.048859	4.815630
232.956584	8000.002453	13.645248	-0.048857	4.815644
233.031820	7999.953512	13.650253	-0.048871	4.815629
233.206507	7999.941410	13.655258	-0.048904	4.815625
232.951577	7999.949037	13.660263	-0.048856	4.815628
233.194997	7999.977546	13.665267	-0.048902	4.815635
233.096541	7999.980235	13.670272	-0.048884	4.815636
232.977115	7999.926006	13.675277	-0.048862	4.815621
233.071157	7999.930745	13.680282	-0.048879	4.815622
233.078289	7999.960764	13.685287	-0.048881	4.815631
233.059363	8000.003171	13.690291	-0.048877	4.815643
233.120427	8000.028727	13.695296	-0.048889	4.815651
232.988337	7999.962551	13.700301	-0.048865	4.815632
233.144975	7999.987518	13.705306	-0.048894	4.815638
232.957748	7999.940732	13.710311	-0.048859	4.815626
232.996672	7999.944578	13.715315	-0.048867	4.815626
233.167190	7999.970838	13.720320	-0.048898	4.815633
232.962497	7999.929107	13.725325	-0.048860	4.815622
233.203347	7999.973586	13.730330	-0.048906	4.815634
233.161883	7999.950510	13.735335	-0.048898	4.815627
233.257673	7999.942468	13.740339	-0.048916	4.815625
233.168161	7999.986934	13.745344	-0.048899	4.815638
233.057343	7999.906158	13.750349	-0.048879	4.815615
233.258073	7999.968135	13.755354	-0.048916	4.815632
233.079537	7999.946042	13.760359	-0.048883	4.815626
233.146322	7999.893762	13.765363	-0.048896	4.815611
233.171306	7999.973175	13.770368	-0.048901	4.815634
233.069137	7999.943779	13.775373	-0.048882	4.815626
233.122151	7999.971338	13.780378	-0.048892	4.815634
233.210238	7999.910863	13.785383	-0.048908	4.815616
233.330462	7999.897879	13.790387	-0.048931	4.815611
233.136889	7999.972685	13.795392	-0.048895	4.815634
233.151423	7999.916356	13.800397	-0.048898	4.815617
233.355073	7999.952760	13.805402	-0.048936	4.815627
233.106504	7999.916723	13.810407	-0.048890	4.815618
233.306112	7999.962669	13.815411	-0.048927	4.815630
233.228452	7999.944345	13.820416	-0.048913	4.815625
233.103305	7999.938062	13.825421	-0.048890	4.815624
233.226381	7999.971026	13.830426	-0.048913	4.815633
233.154993	7999.972018	13.835431	-0.048900	4.815634
233.168876	7999.929556	13.840435	-0.048902	4.815621
233.075839	8000.000653	13.845440	-0.048885	4.815642
233.143096	7999.963326	13.850445	-0.048898	4.815631
233.287597	8000.005178	13.855450	-0.048925	4.815643
233.101811	7999.935997	13.860455	-0.048891	4.815623
233.217668	7999.965642	13.865459	-0.048912	4.815631
233.487835	8000.009529	13.870464	-0.048963	4.815643
233.359588	7999.945550	13.875469	-0.048939	4.815625
233.344045	7999.964527	13.880474	-0.048936	4.815631
233.301182	7999.981993	13.885479	-0.048929	4.815636
233.315570	7999.922459	13.890483	-0.048931	4.815618
233.302542	7999.963895	13.895488	-0.048929	4.815631
233.131483	7999.886413	13.900493	-0.048897	4.815609
233.272129	7999.974104	13.905498	-0.048924	4.815634
233.157513	7999.960519	13.910503	-0.048903	4.815630
233.133938	7999.923855	13.915507	-0.048898	4.815620
233.144749	8000.003039	13.920512	-0.048901	4.815643
233.242537	7999.955531	13.925517	-0.048919	4.815628
233.118449	7999.946062	13.930522	-0.048896	4.815626
232.999518	7999.960162	13.935527	-0.048874	4.815631
233.207332	7999.899491	13.940531	-0.048913	4.815612
233.032280	7999.959652	13.945536	-0.048880	4.815631
233.038532	7999.896785	13.950541	-0.048882	4.815612
233.008102	7999.940073	13.955546	-0.048876	4.815625
232.944465	7999.934786	13.960551	-0.048864	4.815624
233.098277	7999.936223	13.965555	-0.048893	4.815623
233.320915	7999.981475	13.970560	-0.048935	4.815636
233.293261	7999.942610	13.975565	-0.048930	4.815624
233.164551	7999.973631	13.980570	-0.048906	4.815634
233.024041	7999.932939	13.985575	-0.048880	4.815623
233.368431	7999.893695	13.990579	-0.048944	4.815610
233.184667	7999.935567	13.995584	-0.048910	4.815623
233.083583	7999.888041	14.000589	-0.048892	4.815609
233.316562	7999.905705	14.005594	-0.048935	4.815613
233.258363	7999.918654	14.010599	-0.048924	4.815617
233.139405	7999.917808	14.015603	-0.048902	4.815618
233.369978	7999.956784	14.020608	-0.048946	4.815628
233.272719	7999.909319	14.025613	-0.048928	4.815615
233.325100	7999.945409	14.030618	-0.048937	4.815625
233.194942	7999.978542	14.035623	-0.048913	4.815635
233.240250	7999.909901	14.040627	-0.048922	4.815615
233.415865	7999.984282	14.045632	-0.048955	4.815636
233.120468	7999.951756	14.050637	-0.048900	4.815628
233.231733	7999.916209	14.055642	-0.048921	4.815617
233.227626	7999.908683	14.060647	-0.048920	4.815615
233.095379	7999.872395	14.065651	-0.048896	4.815605
233.391089	7999.998893	14.070656	-0.048951	4.815640
233.366735	7999.892829	14.075661	-0.048947	4.815609
233.401475	7999.976671	14.080666	-0.048953	4.815634
233.216692	7999.905371	14.085671	-0.048919	4.815614
233.348034	7999.874419	14.090675	-0.048944	4.815604
233.211118	7999.952278	14.095680	-0.048918	4.815627
233.229428	7999.932305	14.100685	-0.048922	4.815621
233.125115	7999.931697	14.105690	-0.048903	4.815622
233.309670	7999.906944	14.110695	-0.048937	4.815614
233.367400	7999.889745	14.115699	-0.048948	4.815608
233.264250	7999.938261	14.120704	-0.048929	4.815623
233.084127	7999.897994	14.125709	-0.048896	4.815612
233.410292	7999.960936	14.130714	-0.048956	4.815629
233.360064	7999.986823	14.135719	-0.048947	4.815637
233.600085	7999.886108	14.140723	-0.048992	4.815606
233.301246	7999.991235	14.145728	-0.048937	4.815638
233.151473	7999.894882	14.150733	-0.048909	4.815611
233.207796	7999.957723	14.155738	-0.048919	4.815629
233.257344	7999.935054	14.160743	-0.048929	4.815622
233.129951	7999.911654	14.165747	-0.048905	4.815616
233.184249	7999.916817	14.170752	-0.048916	4.815617
233.210991	7999.950356	14.175757	-0.048921	4.815627
233.448622	7999.986244	14.180762	-0.048965	4.815636
233.322789	7999.943654	14.185767	-0.048942	4.815624
233.304009	7999.959376	14.190771	-0.048938	4.815629
233.451877	7999.914814	14.195776	-0.048966	4.815615
233.334802	7999.885176	14.200781	-0.048944	4.815607
233.301123	7999.905994	14.205786	-0.048938	4.815613
233.376524	7999.937119	14.210791	-0.048953	4.815622
233.388450	7999.937326	14.215795	-0.048955	4.815622
233.308530	7999.988353	14.220800	-0.048940	4.815637
233.333502	7999.928990	14.225805	-0.048945	4.815620
233.244271	7999.414096	14.230810	-0.048928	4.815470

233.232007	7996.041044	14.235815	-0.048924	4.814483
233.194916	7990.621848	14.240819	-0.048914	4.812898
233.295094	7983.948145	14.245824	-0.048928	4.810944
233.123601	7976.614082	14.250829	-0.048892	4.808797
233.047439	7969.034442	14.255834	-0.048873	4.806577
233.001933	7961.176586	14.260839	-0.048859	4.804275
232.992921	7953.333716	14.265843	-0.048853	4.801975
232.916265	7945.356360	14.270848	-0.048833	4.799635
232.849037	7937.424543	14.275853	-0.048816	4.797307
232.917282	7929.425231	14.280858	-0.048823	4.794958
232.866394	7921.398373	14.285863	-0.048809	4.792600
232.923868	7913.324991	14.290867	-0.048814	4.790226
233.036123	7905.446337	14.295872	-0.048830	4.787909
232.872953	7897.380981	14.300877	-0.048795	4.785537
232.879781	7889.451349	14.305882	-0.048791	4.783202
232.832258	7881.406175	14.310887	-0.048777	4.780833
232.859519	7873.394598	14.315891	-0.048777	4.778472
232.757512	7865.437182	14.320896	-0.048753	4.776127
232.542762	7857.340489	14.325901	-0.048708	4.773739
232.824204	7849.380025	14.330906	-0.048755	4.771389
232.611624	7841.322138	14.335911	-0.048711	4.769011
232.519131	7833.400839	14.340915	-0.048688	4.766671
232.506819	7825.355591	14.345920	-0.048681	4.764293
232.265393	7817.440451	14.350925	-0.048631	4.761954
232.205214	7809.350991	14.355930	-0.048615	4.759561
232.259354	7801.421943	14.360935	-0.048620	4.757213
232.348338	7793.365440	14.365939	-0.048631	4.754827
232.308784	7785.296793	14.370944	-0.048619	4.752437
232.272920	7777.303867	14.375949	-0.048607	4.750068
232.321998	7769.346372	14.380954	-0.048611	4.747707
232.211464	7761.317530	14.385959	-0.048586	4.745325
232.173194	7753.346076	14.390963	-0.048573	4.742959
232.073066	7745.345428	14.395968	-0.048550	4.740583
231.803827	7737.337721	14.400973	-0.048495	4.738204
231.903621	7729.336657	14.405978	-0.048508	4.735824
231.950223	7721.330687	14.410983	-0.048512	4.733443
232.120120	7713.307857	14.415987	-0.048538	4.731054
232.087411	7705.281945	14.420992	-0.048527	4.728664
231.909050	7697.335294	14.425997	-0.048489	4.726297
231.906694	7689.327215	14.431002	-0.048483	4.723910
231.734954	7681.322802	14.436007	-0.048446	4.721523
231.614831	7673.331307	14.441011	-0.048419	4.719139
231.685457	7665.377859	14.446016	-0.048427	4.716765
231.808030	7657.298189	14.451021	-0.048445	4.714351
231.708202	7649.331612	14.456026	-0.048421	4.711970
231.647895	7641.256663	14.461031	-0.048405	4.709556
231.506254	7633.312581	14.466035	-0.048373	4.707180
231.565604	7625.294751	14.471040	-0.048379	4.704780
231.355766	7617.284341	14.476045	-0.048335	4.702382
231.523089	7609.316070	14.481050	-0.048361	4.699994
231.460594	7601.341957	14.486055	-0.048345	4.697604
231.365779	7593.283271	14.491059	-0.048322	4.695187
231.463236	7585.305894	14.496064	-0.048335	4.692793
231.242594	7577.223580	14.501069	-0.048289	4.690367
231.230402	7569.308841	14.506074	-0.048281	4.687990
231.129413	7561.269892	14.511079	-0.048258	4.685574
231.216909	7553.294280	14.516083	-0.048269	4.683175
231.210840	7545.336768	14.521088	-0.048263	4.680782
231.080220	7537.283167	14.526093	-0.048233	4.678358
231.140085	7529.305190	14.531098	-0.048239	4.675955
230.910288	7521.203586	14.536103	-0.048191	4.673514
230.847254	7513.084272	14.541107	-0.048175	4.671066
230.900702	7505.218086	14.546112	-0.048180	4.668694
230.790945	7497.229049	14.551117	-0.048154	4.666283
230.803115	7489.277738	14.556122	-0.048151	4.663882
230.954160	7481.266973	14.561127	-0.048174	4.661462
231.027705	7473.235268	14.566131	-0.048183	4.659034
230.799017	7465.303763	14.571136	-0.048135	4.656636
230.773905	7457.195507	14.576141	-0.048126	4.654183
230.759396	7449.209111	14.581146	-0.048118	4.651765
230.683228	7441.196832	14.586151	-0.048099	4.649338
230.669275	7433.223947	14.591155	-0.048091	4.646922
230.584253	7425.219030	14.596160	-0.048070	4.644495
230.734826	7417.238380	14.601165	-0.048093	4.642074
230.765501	7409.231794	14.606170	-0.048094	4.639644
230.392682	7401.266739	14.611175	-0.048019	4.637225
230.394189	7393.225405	14.616179	-0.048014	4.634782
230.288656	7385.227193	14.621184	-0.047990	4.632351
230.222106	7377.124500	14.626189	-0.047972	4.629886
230.244023	7369.232386	14.631194	-0.047971	4.627484
230.248793	7361.172143	14.636199	-0.047967	4.625030
229.957071	7353.225648	14.641203	-0.047908	4.622609
229.917918	7345.177031	14.646208	-0.047895	4.620156
230.015621	7337.181858	14.651213	-0.047909	4.617718
230.159761	7329.198037	14.656218	-0.047930	4.615282
229.892534	7321.199054	14.661223	-0.047875	4.612840
229.925961	7313.139916	14.666227	-0.047877	4.610378
230.167709	7305.195247	14.671232	-0.047917	4.607950
229.932270	7297.148910	14.676237	-0.047868	4.605489
230.015098	7289.227035	14.681242	-0.047878	4.603066
229.813128	7281.184233	14.686247	-0.047835	4.600604
229.852758	7273.194402	14.691251	-0.047838	4.598157
229.772328	7265.194749	14.696256	-0.047818	4.595705
229.888211	7257.117614	14.701261	-0.047834	4.593229
229.719645	7249.119633	14.706266	-0.047798	4.590775
229.394848	7241.101935	14.711271	-0.047732	4.588314
229.787674	7233.069700	14.716275	-0.047800	4.585848
229.747104	7225.178868	14.721280	-0.047788	4.583423
229.539916	7217.137356	14.726285	-0.047744	4.580951
229.383671	7209.189419	14.731290	-0.047710	4.578506
229.432124	7201.155908	14.736295	-0.047714	4.576034
229.509671	7193.133725	14.741299	-0.047723	4.573564
229.417707	7185.150896	14.746304	-0.047701	4.571104
229.531992	7177.103802	14.751309	-0.047717	4.568624
229.384867	7169.139986	14.756314	-0.047685	4.566168
229.108042	7161.121379	14.761319	-0.047628	4.563693
229.293773	7153.155793	14.766323	-0.047658	4.561233
229.437059	7145.161288	14.771328	-0.047679	4.558764
229.120873	7137.161103	14.776333	-0.047615	4.556291
229.181191	7129.143371	14.781338	-0.047622	4.553811
229.291296	7121.100487	14.786343	-0.047637	4.551323
229.029794	7113.105257	14.791347	-0.047583	4.548847
229.004190	7105.130330	14.796352	-0.047573	4.546377
228.935830	7097.117703	14.801357	-0.047556	4.543893
229.143297	7089.162228	14.806362	-0.047589	4.541426
229.118665	7081.118854	14.811367	-0.047580	4.538931
228.928794	7073.137252	14.816371	-0.047539	4.536452
228.903222	7065.153008	14.821376	-0.047529	4.533972
228.684093	7057.095097	14.826381	-0.047483	4.531467
228.673297	7049.088492	14.831386	-0.047476	4.528978
228.720565	7041.139063	14.836391	-0.047480	4.526504
228.500401	7033.114683	14.841395	-0.047434	4.524006
228.435291	7025.161822	14.846400	-0.047417	4.521528
228.467681	7017.099446	14.851405	-0.047418	4.519016
228.490237	7009.174749	14.856410	-0.047417	4.516545
228.482012	7001.084569	14.861415	-0.047410	4.514021
228.328856	6993.025106	14.866419	-0.047377	4.511504
228.577364	6985.042791	14.871424	-0.047418	4.509012
228.443009	6977.053096	14.876429	-0.047388	4.506514
228.502499	6969.070187	14.881434	-0.047394	4.504018
228.331563	6961.097739	14.886439	-0.047357	4.501524
228.193646	6953.040749	14.891443	-0.047326	4.499001
228.191719	6945.119600	14.896448	-0.047321	4.496520
228.274989	6937.071556	14.901453	-0.047331	4.493998
228.363857	6929.085680	14.906458	-0.047343	4.491494
228.123493	6921.031890	14.911463	-0.047293	4.488967
227.962438	6913.073407	14.916467	-0.047258	4.486468
228.009881	6905.096413	14.921472	-0.047262	4.483962
227.806409	6897.093728	14.926477	-0.047219	4.481447
227.834080	6889.092161	14.931482	-0.047219	4.478931
227.845273	6881.075426	14.936487	-0.047216	4.476408
228.071185	6873.037041	14.941491	-0.047253	4.473879
227.972521	6865.037497	14.946496	-0.047230	4.471359
227.762791	6857.011102	14.951501	-0.047185	4.468828
227.849312	6849.052203	14.956506	-0.047196	4.466319
227.684242	6841.058198	14.961511	-0.047161	4.463796
227.606411	6833.042029	14.966515	-0.047141	4.461265
227.682612	6825.075003	14.971520	-0.047150	4.458748
227.551777	6817.015287	14.976525	-0.047121	4.456201
227.476486	6809.044416	14.981530	-0.047102	4.453680
227.607955	6801.005413	14.986535	-0.047121	4.451136
227.589227	6793.041922	14.991539	-0.047113	4.448615
227.461922	6785.043999	14.996544	-0.047084	4.446081
227.412889	6777.011242	15.001549	-0.047070	4.443535
227.718776	6769.035372	15.006554	-0.047122	4.441006
227.420504	6761.028983	15.011559	-0.047061	4.438464
227.348116	6753.022182	15.016563	-0.047042	4.435922
227.522227	6745.038129	15.021568	-0.047070	4.433386
227.194427	6736.957788	15.026573	-0.047004	4.430816
227.053674	6728.969828	15.031578	-0.046972	4.428275
226.966282	6720.953366	15.036583	-0.046951	4.425723
227.142403	6713.001341	15.041587	-0.046979	4.423192
227.065774	6705.008653	15.046592	-0.046960	4.420645
226.993118	6697.018591	15.051597	-0.046941	4.418097
227.019216	6689.002286	15.056602	-0.046941	4.415541
227.006874	6680.988293	15.061607	-0.046933	4.412983
226.895315	6672.945355	15.066611	-0.046907	4.410414
226.838015	6664.976607	15.071616	-0.046892	4.407867
226.871934	6656.933890	15.076621	-0.046893	4.405296
226.807471	6649.028217	15.081626	-0.046876	4.402766
226.784749	6641.000643	15.086631	-0.046867	4.400197
226.740352	6633.035635	15.091635	-0.046853	4.397645
226.711417	6625.016576	15.096640	-0.046843	4.395075
226.601863	6616.999726	15.101645	-0.046817	4.392504
226.379328	6608.986677	15.106650	-0.046771	4.389932
226.569730	6600.996405	15.111655	-0.046801	4.387368
226.381322	6592.948514	15.116659	-0.046761	4.384781
226.663675	6585.004745	15.121664	-0.046809	4.382230
226.636263	6576.984776	15.126669	-0.046799	4.379650
226.514316	6569.043065	15.131674	-0.046771	4.377094
226.307846	6561.005843	15.136679	-0.046727	4.374505
226.384723	6552.995263	15.141683	-0.046737	4.371925
226.442727	6544.987812	15.146688	-0.046742	4.369344
226.161329	6537.033202	15.151693	-0.046685	4.366776
226.160359	6528.981247	15.156698	-0.046680	4.364177
226.414772	6521.063431	15.161703	-0.046722	4.361622
226.349851	6513.011595	15.166707	-0.046705	4.359020
226.134003	6505.056425	15.171712	-0.046660	4.356446
225.932610	6496.931141	15.176717	-0.046617	4.353816
225.946457	6488.897101	15.181722	-0.046614	4.351216
226.034048	6480.902003	15.186727	-0.046626	4.348627
225.927382	6472.928189	15.191731	-0.046601	4.346042
225.910716	6464.959209	15.196736	-0.046593	4.343457
225.713569	6456.975718	15.201741	-0.046551	4.340865
225.841387	6449.014180	15.206746	-0.046570	4.338281
225.749902	6440.991932	15.211751	-0.046548	4.335674
225.565489	6432.955450	15.216755	-0.046508	4.333061
225.507546	6424.975821	15.221760	-0.046492	4.330465
225.368355	6416.968281	15.226765	-0.046461	4.327858
225.593857	6408.942161	15.231770	-0.046498	4.325245
225.408550	6400.974108	15.236775	-0.046459	4.322648
225.456279	6392.945335	15.241779	-0.046462	4.320030
225.484547	6385.057704	15.246784	-0.046463	4.317457
225.337308	6376.961796	15.251789	-0.046430	4.314813
225.512987	6368.934107	15.256794	-0.046458	4.312192
225.473046	6360.938257	15.261799	-0.046445	4.309578
225.388290	6352.932119	15.266803	-0.046425	4.306959
225.581726	6344.943332	15.271808	-0.046455	4.304346
225.449606	6336.973826	15.276813	-0.046426	4.301736
225.301910	6328.948631	15.281818	-0.046393	4.299105
225.111424	6320.993244	15.286823	-0.046353	4.296495
225.219668	6312.927909	15.291827	-0.046368	4.293850
225.295518	6304.926312	15.296832	-0.046377	4.291225
224.898375	6296.934769	15.301837	-0.046298	4.288596
225.108817	6288.922531	15.306842	-0.046332	4.285965
225.037468	6280.970696	15.311847	-0.046314	4.283349
225.066946	6272.932017	15.316851	-0.046314	4.280704
224.908451	6265.005521	15.321856	-0.046280	4.278093
224.962096	6256.918331	15.326861	-0.046284	4.275429
224.930675	6248.943478	15.331866	-0.046274	4.272800
224.753433	6240.901710	15.336871	-0.046235	4.270145
224.992023	6232.916380	15.341875	-0.046275	4.267512
224.981229	6224.871693	15.346880	-0.046268	4.264855
224.711487	6216.940056	15.351885	-0.046213	4.262231
224.623174	6208.954699	15.356890	-0.046191	4.259589
224.466083	6200.956412	15.361895	-0.046157	4.256941
224.644805	6192.935077	15.366899	-0.046185	4.254287
224.722147	6184.933739	15.371904	-0.046194	4.251637
224.529094	6176.880899	15.376909	-0.046153	4.248965
224.420230	6168.928689	15.381914	-0.046128	4.246326
224.235786	6160.930959	15.386919	-0.046089	4.243670
224.224647	6152.962509	15.391923	-0.046081	4.241023
224.270791	6144.997402	15.396928	-0.046085	4.238376
224.143629	6136.966250	15.401933	-0.046056	4.235704
224.104160	6128.932986	15.406938	-0.046044	4.233030
224.139674	6120.891379	15.411943	-0.046045	4.230353
224.037676	6112.946019	15.416947	-0.046021	4.227704
224.088594	6104.927200	15.421952	-0.046026	4.225031
224.122475	6096.947628	15.426957	-0.046027	4.222369
224.173436	6088.931434	15.431962	-0.046031	4.219694
223.977692	6081.010923	15.436967	-0.045990	4.217046
223.923475	6072.962314	15.441971	-0.045975	4.214355
224.087080	6064.948596	15.446976	-0.046000	4.211677
223.920309	6056.931448	15.451981	-0.045964	4.208992
223.831459	6048.927326	15.456986	-0.045942	4.206310
223.771466	6040.987056	15.461991	-0.045926	4.203649
223.728693	6032.939617	15.466995	-0.045913	4.200950
223.733292	6024.973080	15.472000	-0.045909	4.198277
223.629507	6016.969519	15.477005	-0.045885	4.195588
223.672488	6008.882840	15.482010	-0.045887	4.192872
223.424648	6000.884087	15.487015	-0.045836	4.190180
223.423055	5992.882611	15.492019	-0.045831	4.187488
223.564917	5984.905723	15.497024	-0.045852	4.184805
223.557394	5976.922117	15.502029	-0.045846	4.182115
223.297749	5968.942704	15.507034	-0.045792	4.179423
223.259776	5960.976004	15.512039	-0.045780	4.176735
223.306798	5952.902502	15.517043	-0.045784	4.174011
223.387925	5944.912592	15.522048	-0.045794	4.171314
223.043217	5936.909860	15.527053	-0.045725	4.168605
223.165929	5928.925235	15.532058	-0.045743	4.165907
223.091280	5920.943250	15.537063	-0.045724	4.163205
223.199258	5912.931645	15.542067	-0.045739	4.160494
223.193201	5904.955873	15.547072	-0.045733	4.157791
222.992187	5896.901848	15.552077	-0.045690	4.155058
223.017802	5888.926258	15.557082	-0.045690	4.152353
223.054014	5880.887462	15.562087	-0.045691	4.149624
222.985130	5872.889808	15.567091	-0.045674	4.146906
222.981019	5864.949303	15.572096	-0.045668	4.144207
222.769593	5856.936045	15.577101	-0.045623	4.141479
222.925568	5848.931493	15.582106	-0.045647	4.138756
222.820604	5840.920483	15.587111	-0.045623	4.136026
222.798909	5832.906300	15.592115	-0.045614	4.133294
222.812221	5824.897987	15.597120	-0.045611	4.130563
222.693686	5816.886998	15.602125	-0.045584	4.127828
222.781914	5808.881988	15.607130	-0.045595	4.125095
222.715411	5800.960128	15.612135	-0.045578	4.122387
222.512349	5792.922641	15.617139	-0.045535	4.119636
222.733781	5784.981448	15.622144	-0.045571	4.116921
222.374907	5776.916835	15.627149	-0.045499	4.114155
222.614102	5768.870725	15.632154	-0.045539	4.111401
222.420226	5760.880951	15.637159	-0.045497	4.108659
222.090175	5752.867232	15.642163	-0.045431	4.105905
222.384597	5744.933243	15.647168	-0.045481	4.103185
222.323739	5736.888203	15.652173	-0.045464	4.100420
222.347812	5728.934291	15.657178	-0.045464	4.097686
222.286253	5720.917354	15.662183	-0.045447	4.094927
222.216151	5712.923411	15.667187	-0.045429	4.092174
222.202284	5704.910930	15.672192	-0.045422	4.089414
222.137501	5696.962014	15.677197	-0.045404	4.086673
222.156358	5688.933718	15.682202	-0.045403	4.083903
222.025391	5680.979231	15.687207	-0.045373	4.081156
221.908205	5672.964557	15.692211	-0.045347	4.078385
222.048447	5664.986542	15.697216	-0.045368	4.075630
221.861916	5656.918834	15.702221	-0.045328	4.072836
221.927300	5648.906003	15.707226	-0.045335	4.070064
221.906831	5640.930954	15.712231	-0.045326	4.067301
221.892475	5632.923271	15.717235	-0.045318	4.064525
221.886060	5624.997226	15.722240	-0.045312	4.061776
221.787163	5616.974288	15.727245	-0.045289	4.058990
221.604831	5608.994527	15.732250	-0.045250	4.056216
221.764895	5600.952104	15.737255	-0.045274	4.053423
221.740364	5592.924719	15.742259	-0.045265	4.050631
221.798262	5584.977418	15.747264	-0.045270	4.047865
221.555116	5576.962279	15.752269	-0.045220	4.045070
221.523610	5568.989437	15.757274	-0.045209	4.042291
221.339701	5560.965984	15.762279	-0.045170	4.039490
221.360665	5553.001963	15.767283	-0.045169	4.036711
221.391975	5544.933960	15.772288	-0.045169	4.033893
221.137427	5536.845595	15.777293	-0.045117	4.031063
221.192226	5528.900346	15.782298	-0.045122	4.028285
221.257116	5520.878972	15.787303	-0.045129	4.025478
221.041975	5512.916478	15.792307	-0.045084	4.022686
221.238992	5504.960103	15.797312	-0.045116	4.019901
221.127319	5496.972140	15.802317	-0.045090	4.017098
221.016288	5488.935535	15.807322	-0.045064	4.014275
220.950854	5480.932806	15.812327	-0.045047	4.011464
220.824415	5472.919818	15.817331	-0.045018	4.008646
220.817113	5464.955063	15.822336	-0.045012	4.005844
220.893469	5456.951308	15.827341	-0.045021	4.003028
220.983165	5448.953438	15.832346	-0.045033	4.000213
220.812034	5441.006741	15.837351	-0.044996	3.997409
220.754312	5432.979084	15.842355	-0.044980	3.994577
220.851620	5424.969456	15.847360	-0.044993	3.991752
220.571087	5416.917573	15.852365	-0.044936	3.988903
220.589874	5408.916809	15.857370	-0.044934	3.986076
220.517810	5400.937432	15.862375	-0.044916	3.983252
220.507355	5392.952927	15.867379	-0.044909	3.980426
220.561844	5385.021269	15.872384	-0.044914	3.977617
220.344656	5376.977730	15.877389	-0.044868	3.974762
220.334957	5368.964533	15.882394	-0.044861	3.971920
220.452146	5360.948400	15.887399	-0.044878	3.969076
220.401828	5352.945983	15.892403	-0.044864	3.966233
220.387855	5345.001141	15.897408	-0.044856	3.963408
220.371612	5336.993655	15.902413	-0.044848	3.960560
220.153313	5329.042931	15.907418	-0.044802	3.957725
220.089889	5321.042290	15.912423	-0.044785	3.954874
219.860500	5312.974142	15.917427	-0.044738	3.951994
219.906893	5304.975443	15.922432	-0.044741	3.949141
219.769398	5296.969705	15.927437	-0.044711	3.946280
219.798844	5288.985176	15.932442	-0.044711	3.943428
219.777365	5281.014179	15.937447	-0.044702	3.940577
219.647021	5273.023858	15.942451	-0.044673	3.937716
219.582493	5265.031759	15.947456	-0.044656	3.934853
219.736321	5256.997106	15.952461	-0.044679	3.931977
219.825394	5248.975015	15.957466	-0.044691	3.929102
219.425273	5241.040895	15.962471	-0.044611	3.926247
219.684662	5233.003646	15.967475	-0.044654	3.923366
219.914416	5225.050126	15.972480	-0.044692	3.920512
219.554228	5217.069127	15.977485	-0.044620	3.917635
219.536768	5209.020197	15.982490	-0.044612	3.914738
219.764076	5201.009684	15.987495	-0.044649	3.911857
219.710438	5192.990074	15.992499	-0.044634	3.908965
219.810083	5185.009135	15.997504	-0.044647	3.906088
219.609996	5177.004699	16.002509	-0.044605	3.903195
219.529863	5169.025070	16.007514	-0.044585	3.900311
219.329428	5161.074964	16.012519	-0.044543	3.897433
219.311083	5153.024615	16.017523	-0.044534	3.894520
219.450476	5145.019371	16.022528	-0.044555	3.891624
219.180939	5137.029675	16.027533	-0.044500	3.888724
219.104160	5129.027187	16.032538	-0.044481	3.885821
219.282159	5121.062682	16.037543	-0.044509	3.882935
219.223932	5113.036779	16.042547	-0.044493	3.880019
219.209204	5105.053242	16.047552	-0.044485	3.877117
219.105680	5097.004979	16.052557	-0.044461	3.874188
219.027250	5088.793432	16.057562	-0.044441	3.871198
218.939566	5080.890365	16.062567	-0.044419	3.868318
218.779363	5072.897874	16.067571	-0.044385	3.865401
218.987444	5064.991399	16.072576	-0.044418	3.862521
218.787385	5056.978973	16.077581	-0.044376	3.859592
218.586376	5049.028298	16.082586	-0.044334	3.856683
218.729977	5041.026215	16.087591	-0.044355	3.853760
218.742089	5033.023810	16.092595	-0.044352	3.850833
218.792468	5025.009164	16.097600	-0.044357	3.847899
218.665990	5016.969638	16.102605	-0.044328	3.844950
218.566816	5009.070959	16.107610	-0.044305	3.842051
218.459401	5001.063962	16.112615	-0.044280	3.839110
218.428542	4993.115750	16.117619	-0.044269	3.836190
218.552435	4985.070589	16.122624	-0.044287	3.833236
218.623373	4977.027812	16.127629	-0.044295	3.830279
218.438015	4969.111827	16.132634	-0.044255	3.827361
218.531943	4961.072450	16.137639	-0.044268	3.824401
218.469963	4953.108325	16.142643	-0.044251	3.821463
218.411645	4945.101092	16.147648	-0.044235	3.818507
218.299151	4937.115904	16.152653	-0.044209	3.815556
218.348958	4929.107254	16.157658	-0.044213	3.812597
218.396552	4921.087215	16.162663	-0.044217	3.809632
218.150963	4913.104042	16.167667	-0.044166	3.806671
218.209875	4905.151447	16.172672	-0.044172	3.803727
217.998301	4897.157779	16.177677	-0.044128	3.800759
217.841053	4889.159675	16.182682	-0.044094	3.797788
217.750430	4881.145465	16.187687	-0.044072	3.794810
217.845680	4873.080352	16.192691	-0.044084	3.791815
217.783024	4865.099804	16.197696	-0.044068	3.788846
217.926814	4857.073783	16.202701	-0.044089	3.785862
217.870991	4849.117124	16.207706	-0.044074	3.782897
217.820612	4841.139616	16.212711	-0.044059	3.779922
217.708292	4833.126987	16.217715	-0.044033	3.776930
217.600610	4825.166453	16.222720	-0.044008	3.773955
217.822416	4817.088652	16.227725	-0.044045	3.770942
217.812320	4809.098957	16.232730	-0.044038	3.767954
217.745610	4801.109069	16.237735	-0.044020	3.764962
217.559725	4793.141214	16.242739	-0.043981	3.761973
217.657348	4785.191459	16.247744	-0.043994	3.758996
217.407828	4777.171250	16.252749	-0.043942	3.755981
217.433663	4769.140534	16.257754	-0.043942	3.752966
217.408974	4761.121067	16.262759	-0.043932	3.749952
217.236964	4753.148783	16.267763	-0.043895	3.746950
217.481011	4745.168557	16.272768	-0.043936	3.743952
217.135487	4737.166986	16.277773	-0.043866	3.740930
217.033301	4729.200599	16.282778	-0.043842	3.737925
217.074382	4721.200195	16.287783	-0.043845	3.734907
216.951119	4713.185243	16.292787	-0.043817	3.731878
217.224585	4705.175611	16.297792	-0.043863	3.728858
217.021877	4697.156481	16.302797	-0.043820	3.725820
217.233947	4689.225489	16.307802	-0.043854	3.722823
217.121453	4681.232626	16.312807	-0.043828	3.719793
216.981509	4673.253034	16.317811	-0.043797	3.716764
216.820845	4665.227890	16.322816	-0.043762	3.713715
216.618231	4657.114336	16.327821	-0.043719	3.710629
216.656334	4649.141451	16.332826	-0.043721	3.707600
216.437824	4641.190946	16.337831	-0.043676	3.704570
216.517981	4633.193948	16.342835	-0.043685	3.701528
216.653210	4625.233473	16.347840	-0.043706	3.698498
216.384315	4617.239703	16.352845	-0.043650	3.695443
216.587798	4609.239560	16.357850	-0.043683	3.692395
216.673116	4601.227595	16.362855	-0.043694	3.689337
216.479234	4593.276649	16.367859	-0.043653	3.686293
216.483824	4585.305315	16.372864	-0.043649	3.683244
216.403118	4577.257431	16.377869	-0.043629	3.680160
216.335244	4569.278180	16.382874	-0.043611	3.677100
216.190506	4561.298550	16.387879	-0.043579	3.674036
216.345281	4553.225041	16.392883	-0.043603	3.670941
216.341563	4545.276991	16.397888	-0.043597	3.667887
215.941284	4537.275521	16.402893	-0.043517	3.664800
216.033029	4529.298722	16.407898	-0.043529	3.661733
216.081907	4521.286113	16.412903	-0.043533	3.658648
216.034989	4513.285155	16.417907	-0.043520	3.655563
216.211032	4505.280594	16.422912	-0.043547	3.652479
216.143205	4497.258217	16.427917	-0.043530	3.649380
216.006501	4489.295874	16.432922	-0.043499	3.646299
215.922278	4481.317347	16.437927	-0.043478	3.643210
215.875513	4473.302734	16.442931	-0.043465	3.640107
215.958787	4465.343155	16.447936	-0.043475	3.637025
215.721848	4457.306321	16.452941	-0.043426	3.633902
215.913631	4449.273160	16.457946	-0.043457	3.630789
215.828556	4441.298291	16.462951	-0.043436	3.627689
215.677549	4433.261059	16.467955	-0.043403	3.624560
215.708421	4425.370433	16.472960	-0.043403	3.621491
215.501414	4417.344596	16.477965	-0.043360	3.618359
215.482031	4409.350975	16.482970	-0.043351	3.615243
215.497958	4401.344161	16.487975	-0.043349	3.612120
215.480081	4393.339480	16.492979	-0.043341	3.608994
215.470109	4385.366736	16.497984	-0.043334	3.605878
215.347688	4377.388184	16.502989	-0.043306	3.602753
215.277311	4369.405711	16.507994	-0.043288	3.599626
215.443119	4361.458645	16.512999	-0.043313	3.596517
215.305129	4353.407371	16.518003	-0.043283	3.593356
215.089546	4345.421326	16.523008	-0.043237	3.590215
215.321561	4337.390900	16.528013	-0.043276	3.587067
215.332881	4329.412811	16.533018	-0.043273	3.583930
215.232812	4321.455365	16.538023	-0.043249	3.580796
215.091390	4313.456459	16.543027	-0.043218	3.577641
215.301517	4305.444494	16.548032	-0.043252	3.574488
214.957513	4297.465137	16.553037	-0.043183	3.571330
214.860984	4289.454252	16.558042	-0.043160	3.568163
214.901969	4281.451437	16.563047	-0.043162	3.565001
214.846684	4273.483335	16.568051	-0.043147	3.561847
214.848668	4265.492859	16.573056	-0.043142	3.558683
214.651163	4257.499127	16.578061	-0.043100	3.555508
214.613091	4249.396127	16.583066	-0.043088	3.552293
214.489014	4241.419298	16.588071	-0.043060	3.549122
214.358375	4233.423453	16.593075	-0.043031	3.545940
214.602068	4225.439683	16.598080	-0.043071	3.542772
214.436615	4217.457704	16.603085	-0.043035	3.539589
214.291357	4209.499472	16.608090	-0.043003	3.536413
214.286386	4201.490116	16.613095	-0.042997	3.533218
214.297882	4193.461749	16.618099	-0.042994	3.530013
214.253551	4185.515205	16.623104	-0.042981	3.526837
214.123327	4177.512955	16.628109	-0.042951	3.523632
214.336684	4169.513605	16.633114	-0.042986	3.520437
214.199267	4161.560776	16.638119	-0.042955	3.517246
214.206955	4153.534827	16.643123	-0.042952	3.514028
214.383969	4145.500078	16.648128	-0.042980	3.510808
214.224877	4137.519553	16.653133	-0.042945	3.507597
214.058103	4129.518298	16.658138	-0.042909	3.504374
214.056762	4121.594598	16.663143	-0.042904	3.501184
214.113239	4113.566735	16.668147	-0.042909	3.497952
213.961827	4105.615109	16.673152	-0.042876	3.494740
213.739590	4097.606825	16.678157	-0.042829	3.491501
214.036357	4089.571572	16.683162	-0.042880	3.488264
214.087394	4081.608486	16.688167	-0.042884	3.485046
213.738964	4073.651056	16.693171	-0.042814	3.481814
213.857795	4065.652725	16.698176	-0.042831	3.478577
213.629453	4057.689271	16.703181	-0.042784	3.475341
213.299896	4049.654504	16.708186	-0.042717	3.472069
213.553522	4041.609492	16.713191	-0.042759	3.468808
213.615167	4033.617169	16.718195	-0.042766	3.465560
213.429874	4025.667387	16.723200	-0.042726	3.462318
213.392095	4017.645154	16.728205	-0.042714	3.459049
213.486813	4009.687222	16.733210	-0.042727	3.455807
213.546620	4001.658497	16.738215	-0.042733	3.452531
213.350432	3993.632826	16.743219	-0.042691	3.449246
213.308456	3985.694745	16.748224	-0.042678	3.445998
213.159617	3977.726339	16.753229	-0.042646	3.442731
213.126696	3969.731014	16.758234	-0.042634	3.439454
213.100567	3961.748864	16.763239	-0.042625	3.436179
213.067154	3953.684481	16.768243	-0.042613	3.432867
213.192679	3945.704494	16.773248	-0.042632	3.429592
212.948763	3937.737359	16.778253	-0.042581	3.426307
212.990637	3929.734768	16.783258	-0.042584	3.423014
212.906339	3921.762382	16.788263	-0.042563	3.419725
212.794195	3913.789419	16.793267	-0.042537	3.416433
212.918074	3905.785756	16.798272	-0.042555	3.413132
212.845522	3897.743426	16.803277	-0.042537	3.409805
212.559272	3889.812752	16.808282	-0.042478	3.406515
212.598352	3881.807735	16.813287	-0.042480	3.403201
212.631563	3873.817766	16.818291	-0.042482	3.399890
212.712074	3865.869208	16.823296	-0.042492	3.396595
212.501372	3857.806285	16.828301	-0.042447	3.393239
212.511901	3849.769595	16.833306	-0.042444	3.389898
212.322697	3841.799671	16.838311	-0.042404	3.386574
212.256086	3833.804074	16.843315	-0.042386	3.383241
212.435229	3825.841956	16.848320	-0.042415	3.379928
212.225225	3817.878763	16.853325	-0.042371	3.376596
212.287329	3809.867498	16.858330	-0.042377	3.373251
212.150335	3801.883385	16.863335	-0.042347	3.369907
212.096290	3793.875573	16.868339	-0.042331	3.366553
212.190866	3785.898027	16.873344	-0.042344	3.363214
211.932442	3777.914063	16.878349	-0.042291	3.359855
212.044447	3769.941977	16.883354	-0.042307	3.356512
212.281514	3761.912796	16.888359	-0.042346	3.353146
211.905128	3753.903846	16.893363	-0.042271	3.349762
212.096001	3745.936229	16.898368	-0.042301	3.346414
212.027396	3737.933913	16.903373	-0.042283	3.343038
212.046025	3729.940994	16.908378	-0.042282	3.339665
211.975705	3721.979419	16.913383	-0.042263	3.336299
211.810643	3713.938273	16.918387	-0.042228	3.332893
211.797308	3705.953314	16.923392	-0.042220	3.329513
211.636521	3697.985748	16.928397	-0.042185	3.326130
211.730300	3690.011308	16.933402	-0.042198	3.322752
211.806895	3682.028816	16.938407	-0.042207	3.319365
211.635398	3674.044811	16.943411	-0.042170	3.315965
211.650103	3666.020306	16.948416	-0.042167	3.312552
211.674692	3658.000994	16.953421	-0.042167	3.309137
211.527857	3650.029363	16.958426	-0.042135	3.305733
211.577243	3642.058749	16.963431	-0.042139	3.302333
211.633642	3634.060637	16.968435	-0.042144	3.298918
211.479516	3626.098402	16.973440	-0.042110	3.295507
211.152878	3618.112602	16.978445	-0.042045	3.292076
211.230345	3610.098198	16.983450	-0.042054	3.288644
211.216839	3602.139606	16.988455	-0.042046	3.285229
211.253082	3594.136849	16.993459	-0.042048	3.281794
211.099381	3586.165466	16.998464	-0.042014	3.278361
211.046962	3578.157066	17.003469	-0.042000	3.274912
211.223393	3570.153699	17.008474	-0.042027	3.271471
211.049960	3562.168854	17.013479	-0.041990	3.268021
210.988503	3554.152668	17.018483	-0.041974	3.264557
211.063703	3546.209767	17.023488	-0.041983	3.261128
210.974293	3538.216000	17.028493	-0.041961	3.257666
210.949050	3530.197503	17.033498	-0.041951	3.254192
210.938808	3522.212111	17.038503	-0.041944	3.250729
210.602667	3514.224339	17.043507	-0.041876	3.247249
210.687130	3506.232246	17.048512	-0.041887	3.243780
210.615126	3498.265320	17.053517	-0.041869	3.240311
210.729226	3490.286093	17.058522	-0.041885	3.236841
210.614781	3482.259333	17.063527	-0.041858	3.233338
210.577228	3474.217714	17.068531	-0.041846	3.229827
210.602724	3466.261108	17.073536	-0.041846	3.226352
210.466967	3458.260385	17.078541	-0.041816	3.222848
210.326197	3450.292423	17.083546	-0.041785	3.219354
210.505211	3442.322334	17.088551	-0.041813	3.215868
210.425552	3434.311927	17.093555	-0.041793	3.212350
210.311617	3426.349092	17.098560	-0.041767	3.208848
210.135145	3418.364028	17.103565	-0.041729	3.205330
210.207469	3410.396838	17.108570	-0.041737	3.201825
210.227489	3402.410736	17.113575	-0.041736	3.198307
210.117229	3394.423185	17.118579	-0.041710	3.194778
210.123329	3386.432003	17.123584	-0.041706	3.191249
210.072235	3378.404318	17.128589	-0.041692	3.187698
210.018758	3370.398523	17.133594	-0.041677	3.184152
210.052764	3362.473551	17.138599	-0.041678	3.180641
210.028554	3354.437013	17.143603	-0.041669	3.177075
209.851465	3346.486069	17.148608	-0.041631	3.173536
209.789669	3338.462074	17.153613	-0.041614	3.169966
209.918875	3330.478443	17.158618	-0.041633	3.166418
209.664668	3322.517060	17.163623	-0.041581	3.162859
209.569579	3314.529028	17.168627	-0.041558	3.159291
209.828296	3306.556855	17.173632	-0.041601	3.155742
209.605308	3298.553271	17.178637	-0.041554	3.152153
209.481424	3290.521352	17.183642	-0.041526	3.148552
209.510187	3282.551970	17.188647	-0.041527	3.144982
209.371834	3274.596892	17.193651	-0.041496	3.141407
209.402539	3266.634326	17.198656	-0.041496	3.137832
209.267841	3258.611769	17.203661	-0.041466	3.134218
209.220003	3250.615607	17.208666	-0.041452	3.130616
209.258863	3242.628409	17.213671	-0.041455	3.127017
209.090254	3234.672322	17.218675	-0.041418	3.123419
209.218392	3226.671865	17.223680	-0.041437	3.119811
209.135316	3218.709885	17.228685	-0.041416	3.116206
208.940719	3210.712462	17.233690	-0.041375	3.112575
209.300033	3202.689131	17.238695	-0.041437	3.108954
209.005055	3194.710854	17.243699	-0.041377	3.105320
208.862213	3186.758407	17.248704	-0.041345	3.101699
208.745546	3178.779086	17.253709	-0.041319	3.098064
208.730983	3170.774260	17.258714	-0.041311	3.094417
208.764462	3162.793879	17.263719	-0.041312	3.090779
208.788880	3154.778690	17.268723	-0.041311	3.087121
208.877119	3146.796568	17.273728	-0.041323	3.083476
208.725281	3138.820908	17.278733	-0.041290	3.079819
208.705040	3130.881611	17.283738	-0.041281	3.076180
208.793846	3122.816156	17.288743	-0.041292	3.072485
208.537829	3114.792122	17.293747	-0.041239	3.068787
208.517626	3106.842008	17.298752	-0.041231	3.065130
208.515737	3098.869023	17.303757	-0.041225	3.061460
208.597572	3090.882805	17.308762	-0.041235	3.057782
208.573943	3082.912256	17.313767	-0.041226	3.054103
208.215100	3074.932482	17.318771	-0.041154	3.050398
208.494359	3066.955465	17.323776	-0.041201	3.046721
208.404354	3058.970848	17.328781	-0.041179	3.043018
208.109940	3051.003697	17.333786	-0.041119	3.039310
208.197873	3043.041720	17.338791	-0.041131	3.035617
208.308931	3035.011147	17.343795	-0.041146	3.031889
208.328751	3027.033407	17.348800	-0.041145	3.028176
208.195606	3019.019798	17.353805	-0.041115	3.024435
208.145777	3011.064975	17.358810	-0.041101	3.020721
208.121143	3003.111984	17.363815	-0.041091	3.017004
207.872058	2995.128308	17.368819	-0.041040	3.013258
207.922861	2987.108535	17.373824	-0.041044	3.009504
207.950517	2979.111159	17.378829	-0.041044	3.005755
207.717716	2971.164496	17.383834	-0.040996	3.002013
207.819749	2963.189846	17.388839	-0.041010	2.998269
207.821008	2955.182078	17.393843	-0.041005	2.994499
207.783311	2947.173957	17.398848	-0.040993	2.990723
207.673540	2939.200154	17.403853	-0.040967	2.986955
207.751999	2931.213145	17.408858	-0.040977	2.983185
207.664069	2923.249309	17.413863	-0.040956	2.979413
207.249046	2915.302209	17.418867	-0.040873	2.975628
207.409268	2907.289434	17.423872	-0.040898	2.971836
207.289077	2899.291231	17.428877	-0.040871	2.968031
207.217641	2891.311892	17.433882	-0.040852	2.964233
207.224777	2883.380238	17.438887	-0.040849	2.960457
207.136222	2875.378041	17.443891	-0.040827	2.956638
207.167314	2867.402077	17.448896	-0.040828	2.952832
206.925329	2859.377133	17.453901	-0.040778	2.948984
207.027059	2851.380319	17.458906	-0.040792	2.945162
206.866090	2843.453590	17.463911	-0.040757	2.941355
206.785134	2835.469342	17.468915	-0.040736	2.937519
207.092699	2827.451958	17.473920	-0.040789	2.933683
207.050803	2819.438274	17.478925	-0.040776	2.929826
206.906958	2811.510425	17.483930	-0.040744	2.925999
206.959676	2803.519760	17.488935	-0.040749	2.922148
206.795436	2795.554354	17.493939	-0.040713	2.918292
206.930582	2787.572478	17.498944	-0.040733	2.914438
206.617296	2779.495824	17.503949	-0.040670	2.910510
206.714381	2771.523963	17.508954	-0.040683	2.906650
206.748475	2763.581164	17.513959	-0.040684	2.902795
206.451367	2755.605335	17.518963	-0.040624	2.898901
206.549259	2747.649789	17.523968	-0.040637	2.895032
206.459804	2739.653952	17.528973	-0.040615	2.891129
206.238083	2731.696452	17.533978	-0.040569	2.887232
206.107004	2723.732695	17.538983	-0.040540	2.883332
206.334333	2715.712382	17.543987	-0.040577	2.879418
206.517111	2707.740927	17.548992	-0.040606	2.875521
206.300286	2699.758193	17.553997	-0.040560	2.871591
206.179163	2691.764345	17.559002	-0.040533	2.867655
206.287985	2683.777248	17.564007	-0.040548	2.863729
206.078303	2675.812209	17.569011	-0.040504	2.859792
205.851415	2667.901278	17.574016	-0.040457	2.855875
205.934254	2659.867870	17.579021	-0.040467	2.851909
206.046430	2651.869376	17.584026	-0.040483	2.847956
205.882618	2643.920127	17.589031	-0.040447	2.844007
205.602838	2635.956200	17.594035	-0.040390	2.840039
205.851050	2627.976155	17.599040	-0.040431	2.836087
205.757021	2619.980891	17.604045	-0.040409	2.832102
205.640328	2611.993883	17.609050	-0.040382	2.828115
205.848656	2603.994179	17.614055	-0.040416	2.824134
205.585228	2596.025322	17.619059	-0.040362	2.820136
205.568106	2588.078305	17.624064	-0.040353	2.816157
205.506646	2580.077911	17.629069	-0.040337	2.812144
205.273413	2572.108738	17.634074	-0.040288	2.808130
205.352956	2564.111310	17.639079	-0.040298	2.804114
205.421503	2556.137718	17.644083	-0.040306	2.800104
205.486486	2548.179634	17.649088	-0.040313	2.796096
205.339590	2540.187639	17.654093	-0.040281	2.792053
205.087052	2532.228814	17.659098	-0.040229	2.788015
205.214473	2524.253520	17.664103	-0.040247	2.783984
205.012230	2516.285012	17.669107	-0.040205	2.779932
205.210454	2508.309183	17.674112	-0.040236	2.775893
205.228341	2500.288616	17.679117	-0.040235	2.771816
205.109346	2492.334445	17.684122	-0.040207	2.767758
204.949257	2484.372965	17.689127	-0.040173	2.763688
204.779591	2476.412210	17.694131	-0.040136	2.759611
204.934419	2468.443455	17.699136	-0.040160	2.755544
204.876490	2460.381116	17.704141	-0.040144	2.751410
204.762859	2452.402555	17.709146	-0.040118	2.747310
204.729071	2444.448997	17.714151	-0.040106	2.743221
204.701952	2436.465302	17.719155	-0.040096	2.739111
204.756629	2428.509936	17.724160	-0.040101	2.735014
204.599044	2420.510670	17.729165	-0.040067	2.730876
204.700586	2412.530215	17.734170	-0.040081	2.726756
204.431830	2404.627561	17.739175	-0.040026	2.722649
204.326808	2396.633217	17.744179	-0.040001	2.718497
204.728622	2388.623015	17.749184	-0.040071	2.714362
204.400534	2380.677363	17.754189	-0.040005	2.710209
204.110133	2372.727578	17.759194	-0.039946	2.706050
204.199466	2364.751157	17.764199	-0.039957	2.701894
204.349206	2356.739090	17.769203	-0.039980	2.697717
204.181906	2348.798400	17.774208	-0.039944	2.693551
204.168693	2340.786025	17.779213	-0.039936	2.689351
204.131048	2332.849145	17.784218	-0.039924	2.685182
204.194027	2324.883356	17.789223	-0.039931	2.680998
203.966198	2316.945670	17.794227	-0.039884	2.676804
203.987058	2308.944221	17.799232	-0.039883	2.672585
204.010488	2300.934410	17.804237	-0.039882	2.668355
203.917743	2292.950254	17.809242	-0.039860	2.664125
203.800743	2284.994740	17.814247	-0.039833	2.659902
203.828063	2277.022535	17.819251	-0.039833	2.655672
203.663186	2269.055436	17.824256	-0.039797	2.651426
203.704253	2261.066574	17.829261	-0.039800	2.647174
203.835725	2253.090238	17.834266	-0.039819	2.642929
203.737171	2245.141785	17.839271	-0.039796	2.638676
203.513954	2237.192402	17.844275	-0.039749	2.634408
203.570354	2229.194180	17.849280	-0.039755	2.630126
203.459141	2221.231981	17.854285	-0.039729	2.625844
203.456008	2213.270036	17.859290	-0.039723	2.621563
203.397326	2205.321898	17.864295	-0.039707	2.617278
203.264728	2197.343068	17.869299	-0.039677	2.612965
203.150281	2189.358200	17.874304	-0.039651	2.608643
202.870170	2181.410137	17.879309	-0.039594	2.604322
202.922795	2173.427315	17.884314	-0.039599	2.599998
203.027183	2165.475974	17.889319	-0.039613	2.595687
202.910478	2157.334904	17.894323	-0.039586	2.591251
202.970332	2149.341431	17.899328	-0.039592	2.586899
202.948645	2141.415034	17.904333	-0.039583	2.582572
202.981184	2133.474863	17.909338	-0.039584	2.578233
202.941456	2125.522952	17.914343	-0.039572	2.573875
202.687079	2117.554437	17.919347	-0.039519	2.569487
202.842632	2109.614065	17.924352	-0.039543	2.565134
202.667266	2101.680176	17.929357	-0.039506	2.560755
202.664892	2093.725891	17.934362	-0.039500	2.556368
202.602268	2085.755057	17.939367	-0.039484	2.551961
202.467972	2077.778658	17.944371	-0.039454	2.547539
202.687051	2069.783616	17.949376	-0.039489	2.543123
202.695943	2061.822078	17.954381	-0.039486	2.538703
202.555185	2053.869090	17.959386	-0.039455	2.534270
202.422455	2045.920396	17.964391	-0.039425	2.529831
202.376263	2037.940562	17.969395	-0.039411	2.525374
202.453023	2029.982231	17.974400	-0.039421	2.520930
202.176633	2022.060100	17.979405	-0.039364	2.516472
202.223057	2014.045077	17.984410	-0.039368	2.511978
202.256722	2006.071252	17.989415	-0.039369	2.507498
202.101568	1998.099716	17.994419	-0.039335	2.502998
202.021355	1990.173013	17.999424	-0.039315	2.498520
202.014829	1982.185082	18.004429	-0.039309	2.494005
201.960781	1974.196558	18.009434	-0.039294	2.489478
201.850903	1966.279599	18.014439	-0.039268	2.484979
201.781509	1958.315792	18.019443	-0.039250	2.480449
202.071962	1950.332908	18.024448	-0.039299	2.475926
201.889338	1942.361799	18.029453	-0.039260	2.471366
201.812245	1934.396924	18.034458	-0.039241	2.466809
201.920937	1926.435881	18.039463	-0.039256	2.462260
201.853962	1918.484182	18.044467	-0.039238	2.457694
201.625583	1910.554060	18.049472	-0.039191	2.453120
201.544866	1902.576680	18.054477	-0.039171	2.448522
201.695149	1894.573963	18.059482	-0.039194	2.443918
201.547407	1886.670253	18.064487	-0.039161	2.439340
201.453066	1878.715702	18.069491	-0.039139	2.434727
201.432001	1870.667392	18.074496	-0.039130	2.430057
201.189021	1862.717296	18.079501	-0.039079	2.425419
201.275782	1854.745863	18.084506	-0.039091	2.420784
201.277046	1846.815136	18.089511	-0.039086	2.416157
200.991465	1838.865640	18.094515	-0.039028	2.411489
200.881873	1830.934406	18.099520	-0.039002	2.406835
200.934642	1822.955491	18.104525	-0.039007	2.402158
200.906701	1815.004430	18.109530	-0.038997	2.397481
200.933252	1807.045994	18.114535	-0.038997	2.392795
200.862203	1799.060691	18.119539	-0.038978	2.388076
200.954160	1791.097853	18.124544	-0.038990	2.383374
200.771977	1783.187956	18.129549	-0.038951	2.378673
200.604146	1775.230419	18.134554	-0.038915	2.373935
200.893445	1767.214272	18.139559	-0.038964	2.369189
200.733105	1759.276126	18.144563	-0.038929	2.364444
200.594360	1751.365717	18.149568	-0.038898	2.359707
200.718413	1743.398511	18.154573	-0.038916	2.354949
200.580070	1735.418070	18.159578	-0.038886	2.350151
200.497213	1727.475550	18.164583	-0.038865	2.345372
200.488570	1719.505016	18.169587	-0.038858	2.340571
200.587597	1711.547054	18.174592	-0.038872	2.335777
200.326775	1703.612017	18.179597	-0.038818	2.330957
200.146447	1695.665860	18.184602	-0.038780	2.326128
200.264842	1687.717131	18.189607	-0.038797	2.321311
200.272971	1679.748618	18.194611	-0.038793	2.316463
200.127471	1671.822136	18.199616	-0.038761	2.311618
200.030396	1663.858766	18.204621	-0.038738	2.306744
199.900929	1655.902208	18.209626	-0.038709	2.301861
199.826483	1647.978173	18.214631	-0.038690	2.296993
199.896108	1639.977363	18.219635	-0.038698	2.292079
200.026916	1632.011282	18.224640	-0.038717	2.287181
199.900384	1624.080753	18.229645	-0.038689	2.282272
199.790278	1616.165592	18.234650	-0.038663	2.277364
199.723985	1608.176269	18.239655	-0.038646	2.272403
199.649999	1600.173132	18.244659	-0.038627	2.267422
199.542386	1592.252855	18.249664	-0.038602	2.262479
199.357379	1584.333728	18.254669	-0.038562	2.257518
199.399460	1576.358163	18.259674	-0.038565	2.252532
199.451659	1568.403530	18.264679	-0.038570	2.247548
199.214009	1560.476164	18.269683	-0.038521	2.242545
199.433119	1552.517187	18.274688	-0.038556	2.237550
199.404594	1544.564516	18.279693	-0.038546	2.232527
199.158124	1536.638346	18.284698	-0.038495	2.227490
199.281132	1528.681630	18.289703	-0.038513	2.222455
199.236803	1520.738139	18.294707	-0.038500	2.217402
199.049030	1512.823401	18.299712	-0.038460	2.212343
198.959124	1504.866460	18.304717	-0.038438	2.207254
198.819975	1496.936568	18.309722	-0.038407	2.202167
198.959055	1488.987489	18.314727	-0.038428	2.197080
198.857844	1481.011879	18.319731	-0.038404	2.191943
198.867312	1473.053864	18.324736	-0.038401	2.186815
198.897078	1465.112578	18.329741	-0.038401	2.181687
198.681591	1457.196578	18.334746	-0.038356	2.176541
198.628065	1449.264876	18.339751	-0.038341	2.171388
198.478177	1441.312065	18.344755	-0.038308	2.166200
198.692383	1433.362106	18.349760	-0.038343	2.161035
198.556711	1425.442058	18.354765	-0.038313	2.155845
198.615916	1417.469290	18.359770	-0.038319	2.150626
198.433139	1409.567779	18.364775	-0.038280	2.145418
198.206157	1401.638872	18.369779	-0.038233	2.140175
198.313665	1393.694284	18.374784	-0.038247	2.134941
198.276194	1385.737617	18.379789	-0.038235	2.129672
198.039290	1377.825591	18.384794	-0.038186	2.124400
198.193237	1369.887582	18.389799	-0.038210	2.119136
198.104428	1361.942930	18.394803	-0.038188	2.113830
197.945959	1353.952996	18.399808	-0.038154	2.108475
197.805301	1346.031370	18.404813	-0.038123	2.103153
197.784149	1338.101657	18.409818	-0.038114	2.097823
197.895701	1330.158024	18.414823	-0.038130	2.092484
197.776518	1322.216129	18.419827	-0.038102	2.087110
197.834228	1314.292518	18.424832	-0.038108	2.081751
197.890118	1306.364931	18.429837	-0.038113	2.076376
197.713786	1298.444939	18.434842	-0.038076	2.070969
197.430281	1290.549740	18.439847	-0.038018	2.065554
197.262767	1282.617686	18.444851	-0.037982	2.060111
197.354531	1274.683967	18.449856	-0.037994	2.054679
197.269394	1266.737906	18.454861	-0.037973	2.049206
197.104691	1258.822535	18.459866	-0.037937	2.043731
197.138898	1250.910964	18.464871	-0.037938	2.038264
197.025463	1242.966295	18.469875	-0.037912	2.032745
197.244867	1234.975828	18.474880	-0.037948	2.027213
197.060454	1227.081546	18.479885	-0.037909	2.021691
196.964061	1219.166730	18.484890	-0.037886	2.016149
196.870940	1211.259898	18.489895	-0.037864	2.010597
196.823001	1203.315030	18.494899	-0.037850	2.005008
196.864295	1195.399659	18.499904	-0.037852	1.999434
196.714502	1187.502040	18.504909	-0.037819	1.993836
196.543024	1179.564820	18.509914	-0.037782	1.988192
196.679097	1171.625065	18.514919	-0.037803	1.982563
196.403444	1163.747022	18.519923	-0.037746	1.976918
196.467281	1155.801963	18.524928	-0.037753	1.971246
196.389891	1147.880801	18.529933	-0.037734	1.965558
196.125642	1139.993005	18.534938	-0.037680	1.959858
196.495516	1132.040014	18.539943	-0.037744	1.954163
196.353354	1124.065366	18.544947	-0.037712	1.948381
196.382643	1116.155548	18.549952	-0.037712	1.942646
196.224772	1108.268048	18.554957	-0.037678	1.936891
196.126394	1100.347496	18.559962	-0.037655	1.931100
196.081032	1092.433598	18.564967	-0.037641	1.925303
196.095530	1084.516879	18.569971	-0.037639	1.919493
195.968281	1076.634085	18.574976	-0.037610	1.913675
195.804095	1068.712980	18.579981	-0.037575	1.907806
195.867114	1060.788226	18.584986	-0.037582	1.901942
195.722845	1052.914041	18.589991	-0.037550	1.896074
195.793166	1044.961462	18.594995	-0.037558	1.890154
195.802692	1037.069422	18.600000	-0.037555	1.884253
195.462589	1029.214393	18.605005	-0.037486	1.878322
195.644280	1021.254103	18.610010	-0.037515	1.872352
195.664855	1013.322760	18.615015	-0.037514	1.866367
195.358749	1005.458733	18.620019	-0.037452	1.860375
195.228768	997.574433	18.625024	-0.037423	1.854369
195.340848	989.625693	18.630029	-0.037439	1.848323
195.337948	981.720879	18.635034	-0.037433	1.842277
195.191617	973.870722	18.640039	-0.037401	1.836237
195.110465	965.939089	18.645043	-0.037381	1.830121
195.045558	958.055506	18.650048	-0.037364	1.824023
194.906493	950.180181	18.655053	-0.037333	1.817903
194.959868	942.260058	18.660058	-0.037338	1.811751
195.013678	934.350503	18.665063	-0.037343	1.805585
194.976051	926.460932	18.670067	-0.037331	1.799403
194.940614	918.574322	18.675072	-0.037319	1.793203
194.842110	910.633849	18.680077	-0.037296	1.786930
194.720250	902.745609	18.685082	-0.037268	1.780674
194.753599	894.869644	18.690087	-0.037269	1.774425
194.517762	886.989552	18.695091	-0.037220	1.768117
194.505251	879.117147	18.700096	-0.037213	1.761820
194.562622	871.226793	18.705101	-0.037219	1.755496
194.354796	863.345100	18.710106	-0.037175	1.749121
194.281342	855.474527	18.715111	-0.037156	1.742750
193.903479	847.633031	18.720115	-0.037081	1.736340
194.075777	839.706728	18.725120	-0.037108	1.729907
194.145225	831.823942	18.730125	-0.037116	1.723473
194.068987	823.958825	18.735130	-0.037097	1.717010
193.934557	816.084263	18.740135	-0.037067	1.710508
193.877137	808.191204	18.745139	-0.037051	1.703975
193.769443	800.338791	18.750144	-0.037026	1.697444
193.797412	792.443027	18.755149	-0.037027	1.690870
193.619573	784.586610	18.760154	-0.036988	1.684276
193.735707	776.715058	18.765159	-0.037005	1.677682
193.497464	768.867282	18.770163	-0.036956	1.671035
193.342654	761.007105	18.775168	-0.036922	1.664362
193.536032	753.116946	18.780173	-0.036953	1.657684
193.462817	745.245438	18.785178	-0.036934	1.650958
193.292425	737.413503	18.790183	-0.036898	1.644226
193.375705	729.542127	18.795187	-0.036908	1.637467
193.187028	721.668459	18.800192	-0.036868	1.630640
193.174739	713.785132	18.805197	-0.036861	1.623800
193.003059	705.954409	18.810202	-0.036824	1.616955
193.039694	698.082598	18.815207	-0.036826	1.610075
192.910362	690.241005	18.820211	-0.036797	1.603168
192.800404	682.418153	18.825216	-0.036771	1.596250
192.831114	674.554947	18.830221	-0.036772	1.589286
192.680481	666.717860	18.835226	-0.036739	1.582289
192.660125	658.886327	18.840231	-0.036730	1.575285
192.700314	651.017008	18.845235	-0.036733	1.568224
192.714070	643.185036	18.850240	-0.036730	1.561161
192.470268	635.394863	18.855245	-0.036680	1.554066
192.439732	627.522753	18.860250	-0.036669	1.546895
192.572025	619.678898	18.865255	-0.036689	1.539741
192.372720	611.858851	18.870259	-0.036647	1.532526
192.425762	604.018880	18.875264	-0.036652	1.525296
192.446510	596.206415	18.880269	-0.036651	1.518053
192.379536	588.374412	18.885274	-0.036634	1.510743
192.219122	580.584575	18.890279	-0.036599	1.503423
192.097948	572.769941	18.895283	-0.036571	1.496050
192.055476	564.947259	18.900288	-0.036558	1.488644
192.018661	557.136154	18.905293	-0.036547	1.481214
191.821982	549.352095	18.910298	-0.036505	1.473746
191.956682	541.471512	18.915303	-0.036525	1.466201
191.800334	533.691310	18.920307	-0.036491	1.458666
191.607553	525.912449	18.925312	-0.036450	1.451089
191.552895	518.105790	18.930317	-0.036435	1.443466
191.516269	510.319407	18.935322	-0.036423	1.435826
191.486053	502.528016	18.940327	-0.036413	1.428141
191.261327	494.755649	18.945331	-0.036366	1.420402
191.282595	486.966839	18.950336	-0.036365	1.412644
191.362118	479.154468	18.955341	-0.036375	1.404829
191.017522	471.437900	18.960346	-0.036306	1.396996
191.077960	463.629490	18.965351	-0.036312	1.389094
190.908152	455.862633	18.970355	-0.036276	1.381151
190.886996	448.095018	18.975360	-0.036267	1.373185
190.828155	440.315688	18.980365	-0.036251	1.365155
190.766409	432.569351	18.985370	-0.036235	1.357111
190.944000	424.773583	18.990375	-0.036263	1.349009
190.498731	417.077572	18.995379	-0.036175	1.340854
190.639019	409.307007	19.000384	-0.036196	1.332673
190.477794	401.573164	19.005389	-0.036161	1.324427
190.373513	393.846063	19.010394	-0.036137	1.316147
190.599666	385.944640	19.015399	-0.036174	1.307686
190.367151	378.241844	19.020403	-0.036126	1.299303
190.169191	370.546652	19.025408	-0.036084	1.290879
189.947584	362.859633	19.030413	-0.036038	1.282404
190.124067	355.114969	19.035418	-0.036066	1.273884
190.058441	347.406648	19.040423	-0.036049	1.265301
189.814086	339.736907	19.045427	-0.035999	1.256669
189.744431	332.034604	19.050432	-0.035981	1.247974
189.769750	324.338429	19.055437	-0.035981	1.239243
189.559919	316.662720	19.060442	-0.035937	1.230427
189.486637	308.975202	19.065447	-0.035918	1.221561
189.536870	301.278968	19.070451	-0.035923	1.212645
189.510874	293.603094	19.075456	-0.035913	1.203671
189.388716	285.964861	19.080461	-0.035886	1.194655
189.535028	278.262263	19.085466	-0.035908	1.185548
189.474836	270.629483	19.090471	-0.035892	1.176412
189.034023	263.041250	19.095475	-0.035805	1.167180
189.197167	255.380052	19.100480	-0.035831	1.157911
189.152296	247.718563	19.105485	-0.035817	1.148523
188.805379	240.130049	19.110490	-0.035748	1.139084
188.848235	232.494499	19.115495	-0.035751	1.129591
188.613793	224.911832	19.120499	-0.035703	1.120024
188.558135	217.319641	19.125504	-0.035688	1.110401
188.370616	209.747730	19.130509	-0.035648	1.100691
188.227151	202.175320	19.135514	-0.035616	1.090904
188.358779	194.573880	19.140519	-0.035636	1.081052
188.147451	187.034110	19.145523	-0.035592	1.071113
188.153046	179.460375	19.150528	-0.035588	1.061085
188.239644	171.894758	19.155533	-0.035600	1.050992
188.095799	164.378366	19.160538	-0.035568	1.040813
187.931890	156.887399	19.165543	-0.035533	1.030563
187.746257	149.394024	19.170547	-0.035494	1.020202
187.592259	141.915609	19.175552	-0.035460	1.009763
187.689198	134.412012	19.180557	-0.035473	0.999242
187.384730	126.948433	19.185562	-0.035412	0.988565
187.324202	119.482700	19.190567	-0.035396	0.977830
187.048622	112.059112	19.195571	-0.035340	0.966982
187.018382	104.633890	19.200576	-0.035330	0.956073
187.039868	97.190843	19.205581	-0.035329	0.945024
186.966859	89.795562	19.210586	-0.035311	0.933891
186.840075	82.430951	19.215591	-0.035283	0.922657
186.843501	75.050273	19.220595	-0.035279	0.911295
186.829915	67.691104	19.225600	-0.035271	0.899818
186.663663	60.611117	19.230605	-0.035236	0.888594