Thu Mar 11 18:14:13 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.608684	-0.060735	0.000000	-0.000005	0.723349

0.542925	-0.055518	0.005005	0.000007	0.723337
0.662894	-0.078313	0.010010	-0.000016	0.723334
0.826416	-0.104883	0.015014	-0.000046	0.723340
0.567195	-0.061917	0.020019	0.000002	0.723334
0.598299	-0.065945	0.025024	-0.000004	0.723337
0.551733	-0.059647	0.030029	0.000004	0.723334
0.656459	-0.079251	0.035034	-0.000015	0.723332
0.620661	-0.069178	0.040038	-0.000009	0.723340
0.438759	-0.040535	0.045043	0.000025	0.723332
0.564729	-0.062250	0.050048	0.000001	0.723334
0.637537	-0.073862	0.055053	-0.000013	0.723337
0.521504	-0.055435	0.060058	0.000009	0.723333
0.793472	-0.100914	0.065062	-0.000042	0.723339
0.502170	-0.053868	0.070067	0.000012	0.723330
0.567960	-0.138303	0.075072	-0.000000	0.723188
0.484908	-0.218504	0.080077	0.000015	0.723002
0.500969	-0.222003	0.085082	0.000012	0.723001
0.608494	-0.237609	0.090086	-0.000008	0.723008
0.745866	-0.266567	0.095091	-0.000034	0.723000
0.649342	-0.247593	0.100096	-0.000016	0.723003
0.664824	-0.251546	0.105101	-0.000019	0.723001
0.644153	-0.402531	0.110106	-0.000015	0.722698
0.697241	-0.414452	0.115110	-0.000026	0.722694
0.510101	-0.385310	0.120115	0.000009	0.722686
0.785147	-0.431581	0.125120	-0.000042	0.722691
0.572739	-0.401678	0.130125	-0.000003	0.722676
0.545944	-0.556432	0.135130	0.000002	0.722363
0.617874	-0.566222	0.140134	-0.000012	0.722370
0.485333	-0.547832	0.145139	0.000013	0.722360
0.544377	-0.553737	0.150144	0.000002	0.722369
0.492905	-0.659562	0.155149	0.000011	0.722144
0.457265	-0.692520	0.160154	0.000018	0.722067
0.653549	-0.723778	0.165158	-0.000019	0.722074
0.713664	-0.748512	0.170163	-0.000030	0.722047
0.728016	-0.906880	0.175168	-0.000033	0.721741
0.776202	-0.916138	0.180173	-0.000042	0.721740
0.620747	-0.893067	0.185178	-0.000013	0.721732
0.551006	-0.996213	0.190182	-0.000000	0.721505
0.512631	-1.028212	0.195187	0.000007	0.721429
0.546917	-1.032058	0.200192	-0.000000	0.721433
0.494941	-1.128475	0.205197	0.000010	0.721226
0.358119	-1.160629	0.210202	0.000035	0.721115
0.630219	-1.204244	0.215206	-0.000016	0.721125
0.601821	-1.297714	0.220211	-0.000011	0.720932
0.439769	-1.293813	0.225216	0.000019	0.720883
0.316020	-1.276382	0.230221	0.000042	0.720874
0.323285	-1.449332	0.235226	0.000041	0.720537
0.474580	-1.473225	0.240230	0.000012	0.720543
0.346940	-1.516355	0.245235	0.000036	0.720413
0.369120	-1.615008	0.250240	0.000032	0.720227
0.374041	-1.619098	0.255245	0.000031	0.720221
0.280534	-1.747285	0.260250	0.000048	0.719936
0.431461	-1.791361	0.265254	0.000020	0.719903
0.438201	-1.873375	0.270259	0.000018	0.719744
0.311126	-1.922550	0.275264	0.000042	0.719603
0.280608	-1.954737	0.280269	0.000047	0.719529
0.141170	-2.063719	0.285274	0.000073	0.719265
0.029263	-2.040586	0.290278	0.000094	0.719272
-0.287516	-2.135977	0.295283	0.000153	0.718973
-2.011661	-1.833500	0.300288	0.000474	0.718964
-3.200714	-1.622841	0.305293	0.000695	0.718962
-3.831026	-1.673740	0.310298	0.000812	0.718641
-4.114607	-1.619994	0.315302	0.000864	0.718647
-4.366629	-1.580213	0.320307	0.000911	0.718638
-4.098225	-1.624264	0.325312	0.000861	0.718645
-4.252691	-1.661009	0.330317	0.000890	0.718519
-5.327837	-1.554357	0.335322	0.001090	0.718352
-4.905708	-1.624604	0.340326	0.001011	0.718362
-4.968588	-1.621907	0.345331	0.001022	0.718345
-5.462099	-1.529151	0.350336	0.001114	0.718355
-5.048786	-1.658102	0.355341	0.001037	0.718246
-6.063721	-1.594652	0.360346	0.001226	0.718015
-5.965394	-1.609601	0.365350	0.001207	0.718020
-6.293464	-1.556347	0.370355	0.001268	0.718010
-6.125319	-1.581282	0.375360	0.001237	0.718020
-5.945262	-1.615371	0.380365	0.001203	0.718017
-6.500215	-1.629977	0.385370	0.001306	0.717793
-6.903245	-1.600965	0.390374	0.001381	0.717709
-6.904820	-1.607046	0.395379	0.001381	0.717696
-7.008465	-1.584009	0.400384	0.001400	0.717706
-7.174584	-1.554898	0.405389	0.001431	0.717705
-7.039868	-1.580990	0.410394	0.001406	0.717701
-7.131355	-1.665065	0.415398	0.001423	0.717503
-8.510420	-1.483694	0.420403	0.001679	0.717377
-8.055353	-1.561598	0.425408	0.001594	0.717383
-7.923937	-1.583194	0.430413	0.001570	0.717387
-8.708027	-1.447088	0.435418	0.001716	0.717380
-7.917457	-1.585974	0.440422	0.001568	0.717384
-7.999181	-1.576553	0.445427	0.001583	0.717375
-8.586567	-1.568658	0.450432	0.001693	0.717184
-9.293205	-1.490535	0.455437	0.001824	0.717090
-8.917982	-1.561479	0.460442	0.001754	0.717082
-8.797290	-1.579588	0.465446	0.001731	0.717089
-9.365686	-1.480951	0.470451	0.001837	0.717084
-8.863265	-1.567490	0.475456	0.001743	0.717090
-8.702744	-1.596994	0.480461	0.001713	0.717089
-9.312137	-1.605055	0.485466	0.001826	0.716858
-9.964336	-1.538733	0.490470	0.001948	0.716760
-10.007349	-1.535887	0.495475	0.001956	0.716751
-9.988087	-1.536443	0.500480	0.001952	0.716757
-10.006996	-1.533947	0.505485	0.001955	0.716755
-9.971649	-1.541746	0.510490	0.001948	0.716753
-9.959053	-1.540523	0.515494	0.001946	0.716760
-10.362712	-1.532147	0.520499	0.002021	0.716634
-11.015289	-1.510519	0.525504	0.002142	0.716447
-10.793536	-1.549434	0.530509	0.002101	0.716449
-11.268266	-1.466726	0.535514	0.002189	0.716445
-10.917227	-1.523704	0.540518	0.002123	0.716457
-10.846714	-1.542023	0.545523	0.002110	0.716446
-10.988917	-1.515120	0.550528	0.002136	0.716449
-10.867937	-1.534901	0.555533	0.002114	0.716453
-11.577066	-1.563064	0.560538	0.002246	0.716147
-11.848746	-1.517746	0.565542	0.002296	0.716142
-12.390523	-1.427701	0.570547	0.002397	0.716129
-11.728858	-1.542341	0.575552	0.002273	0.716136
-11.850467	-1.520486	0.580557	0.002296	0.716136
-12.365309	-1.431733	0.585562	0.002391	0.716131
-11.746956	-1.536097	0.590566	0.002276	0.716143
-11.773877	-1.571608	0.595571	0.002281	0.716063
-12.862984	-1.468275	0.600576	0.002484	0.715884
-12.751700	-1.487630	0.605581	0.002463	0.715885
-12.667356	-1.505495	0.610586	0.002447	0.715880
-12.400756	-1.548738	0.615590	0.002397	0.715888
-12.835083	-1.474916	0.620595	0.002478	0.715882
-12.918463	-1.458414	0.625600	0.002493	0.715885
-12.549607	-1.574888	0.630605	0.002424	0.715785
-13.940067	-1.449401	0.635610	0.002683	0.715543
-13.635045	-1.497956	0.640614	0.002626	0.715555
-13.793670	-1.474860	0.645619	0.002655	0.715545
-13.882759	-1.457183	0.650624	0.002672	0.715549
-14.037350	-1.429254	0.655629	0.002700	0.715550
-13.726920	-1.487669	0.660634	0.002642	0.715544
-13.394333	-1.544009	0.665638	0.002580	0.715550
-14.255709	-1.508755	0.670643	0.002741	0.715316
-15.165956	-1.387997	0.675648	0.002910	0.715234
-14.607774	-1.488738	0.680653	0.002806	0.715232
-14.854935	-1.447190	0.685658	0.002852	0.715227
-14.931448	-1.428843	0.690662	0.002866	0.715237
-14.442444	-1.521589	0.695667	0.002775	0.715226
-14.448053	-1.517722	0.700672	0.002775	0.715232
-14.795070	-1.464877	0.705677	0.002840	0.715215
-15.593174	-1.479846	0.710682	0.002988	0.714903
-15.480229	-1.493759	0.715686	0.002967	0.714916
-16.026191	-1.403106	0.720691	0.003069	0.714903
-15.625597	-1.472511	0.725696	0.002994	0.714907
-15.271517	-1.534573	0.730701	0.002928	0.714910
-15.907136	-1.426060	0.735706	0.003046	0.714901
-15.725787	-1.452198	0.740710	0.003012	0.714913
-15.583185	-1.552086	0.745715	0.002985	0.714766
-16.804622	-1.412841	0.750720	0.003212	0.714610
-16.562655	-1.456189	0.755725	0.003167	0.714610
-16.720183	-1.430134	0.760730	0.003196	0.714607
-16.460779	-1.473208	0.765734	0.003148	0.714613
-16.617365	-1.447871	0.770739	0.003177	0.714608
-16.888924	-1.398867	0.775744	0.003227	0.714610
-16.512486	-1.464993	0.780749	0.003157	0.714612
-17.213127	-1.506926	0.785754	0.003287	0.714281
-17.737584	-1.412394	0.790758	0.003385	0.714284
-17.880853	-1.391353	0.795763	0.003411	0.714275
-17.352633	-1.482283	0.800768	0.003313	0.714282
-17.827459	-1.397339	0.805773	0.003401	0.714283
-17.852113	-1.396724	0.810778	0.003405	0.714276
-17.267259	-1.495228	0.815782	0.003296	0.714287
-17.692739	-1.454790	0.820787	0.003375	0.714217
-18.523679	-1.432449	0.825792	0.003530	0.713968
-17.990129	-1.525157	0.830797	0.003431	0.713973
-18.690785	-1.404454	0.835802	0.003561	0.713965
-18.648523	-1.407197	0.840806	0.003553	0.713975
-18.482353	-1.440735	0.845811	0.003522	0.713967
-18.468446	-1.441803	0.850816	0.003519	0.713971
-18.438130	-1.445442	0.855821	0.003513	0.713974
-19.062340	-1.473509	0.860826	0.003629	0.713698
-19.338443	-1.446383	0.865830	0.003680	0.713654
-19.369171	-1.444800	0.870835	0.003686	0.713647
-19.673479	-1.389723	0.875840	0.003742	0.713649
-19.530967	-1.414373	0.880845	0.003716	0.713651
-19.640143	-1.396104	0.885850	0.003736	0.713649
-19.460998	-1.425004	0.890854	0.003702	0.713655
-19.589786	-1.419806	0.895859	0.003726	0.713620
-20.000911	-1.477797	0.900864	0.003803	0.713359
-19.991050	-1.478617	0.905869	0.003801	0.713362
-20.902840	-1.320131	0.910874	0.003970	0.713354
-20.065505	-1.464852	0.915878	0.003814	0.713363
-20.272398	-1.432311	0.920883	0.003852	0.713355
-20.666263	-1.359904	0.925888	0.003926	0.713360
-20.339402	-1.416772	0.930893	0.003865	0.713363
-20.676336	-1.506091	0.935898	0.003927	0.713066
-21.631674	-1.355293	0.940902	0.004105	0.713028
-21.537044	-1.377689	0.945907	0.004087	0.713017
-21.108833	-1.450225	0.950912	0.004007	0.713025
-21.411388	-1.397382	0.955917	0.004063	0.713023
-21.898076	-1.316005	0.960922	0.004154	0.713013
-21.109452	-1.448993	0.965926	0.004007	0.713028
-21.400462	-1.418952	0.970931	0.004061	0.712985
-22.452561	-1.371626	0.975936	0.004256	0.712706
-22.269377	-1.402585	0.980941	0.004222	0.712710
-22.389726	-1.384439	0.985946	0.004244	0.712704
-22.268391	-1.400968	0.990950	0.004222	0.712714
-22.510943	-1.362616	0.995955	0.004267	0.712705
-22.544333	-1.355731	1.000960	0.004273	0.712707
-22.232600	-1.410261	1.005965	0.004215	0.712709
-22.603598	-1.379754	1.010970	0.004283	0.712639
-23.047843	-1.426281	1.015974	0.004366	0.712389
-22.785674	-1.475273	1.020979	0.004317	0.712384
-23.619391	-1.324882	1.025984	0.004472	0.712388
-23.399211	-1.363454	1.030989	0.004431	0.712390
-23.303113	-1.384422	1.035994	0.004413	0.712383
-23.283294	-1.381258	1.040998	0.004409	0.712396
-23.560837	-1.337295	1.046003	0.004460	0.712386
-23.379644	-1.471364	1.051008	0.004427	0.712183
-24.103445	-1.386697	1.056013	0.004561	0.712095
-24.555454	-1.312622	1.061018	0.004645	0.712083
-24.117184	-1.386374	1.066022	0.004563	0.712092
-23.928471	-1.422551	1.071027	0.004528	0.712087
-24.228507	-1.369838	1.076032	0.004584	0.712086
-23.996684	-1.407940	1.081037	0.004540	0.712093
-24.152960	-1.467503	1.086042	0.004569	0.711919
-25.217037	-1.356083	1.091046	0.004767	0.711763
-25.157587	-1.370557	1.096051	0.004756	0.711756
-25.248192	-1.352969	1.101056	0.004773	0.711759
-25.031831	-1.390550	1.106061	0.004732	0.711761
-25.405362	-1.327910	1.111066	0.004802	0.711754
-25.362734	-1.330305	1.116070	0.004794	0.711764
-25.119359	-1.378101	1.121075	0.004748	0.711756
-25.405022	-1.456318	1.126080	0.004801	0.711499
-26.176168	-1.340509	1.131085	0.004945	0.711456
-26.003581	-1.375494	1.136090	0.004912	0.711448
-25.765226	-1.414217	1.141094	0.004868	0.711456
-26.243511	-1.331734	1.146099	0.004957	0.711450
-26.117996	-1.354457	1.151104	0.004933	0.711450
-25.452679	-1.470202	1.156109	0.004809	0.711456
-26.600224	-1.384764	1.161114	0.005023	0.711219
-27.191470	-1.318483	1.166118	0.005132	0.711141
-26.342493	-1.473334	1.171123	0.004974	0.711134
-26.642731	-1.420033	1.176128	0.005030	0.711134
-26.894079	-1.371768	1.181133	0.005077	0.711141
-26.722156	-1.405774	1.186138	0.005044	0.711135
-26.490617	-1.442346	1.191142	0.005001	0.711145
-27.249731	-1.427554	1.196147	0.005142	0.710905
-27.790579	-1.349593	1.201152	0.005243	0.710868
-27.311972	-1.432229	1.206157	0.005154	0.710874
-27.493060	-1.405086	1.211162	0.005187	0.710864
-27.715706	-1.360841	1.216166	0.005228	0.710873
-27.490765	-1.405936	1.221171	0.005186	0.710864
-27.671126	-1.387366	1.226176	0.005220	0.710837
-28.217744	-1.441332	1.231181	0.005321	0.710535
-28.309116	-1.429040	1.236186	0.005338	0.710527
-28.431523	-1.403637	1.241190	0.005361	0.710535
-28.877039	-1.326437	1.246195	0.005444	0.710531
-28.995558	-1.304384	1.251200	0.005465	0.710533
-28.459946	-1.396714	1.256205	0.005366	0.710539
-28.795685	-1.341655	1.261210	0.005428	0.710530
-29.271347	-1.378081	1.266214	0.005516	0.710288
-29.718475	-1.335353	1.271219	0.005599	0.710215
-29.657533	-1.345672	1.276224	0.005588	0.710216
-29.423614	-1.385686	1.281229	0.005544	0.710220
-29.788088	-1.323550	1.286234	0.005612	0.710215
-29.381541	-1.391828	1.291238	0.005536	0.710223
-29.555763	-1.364457	1.296243	0.005568	0.710216
-29.740252	-1.371263	1.301248	0.005602	0.710137
-30.123304	-1.422482	1.306253	0.005674	0.709899
-30.057168	-1.441418	1.311258	0.005661	0.709885
-30.747917	-1.313403	1.316262	0.005790	0.709895
-30.421304	-1.372592	1.321267	0.005729	0.709893
-30.239905	-1.406253	1.326272	0.005695	0.709891
-30.629551	-1.334242	1.331277	0.005767	0.709896
-30.456135	-1.395406	1.336282	0.005735	0.709836
-31.005536	-1.415129	1.341286	0.005837	0.709601
-31.094199	-1.403821	1.346291	0.005853	0.709593
-31.797969	-1.277778	1.351296	0.005984	0.709594
-31.218781	-1.379055	1.356301	0.005876	0.709598
-31.182996	-1.389223	1.361306	0.005869	0.709591
-31.622530	-1.308048	1.366310	0.005951	0.709597
-31.422766	-1.347401	1.371315	0.005913	0.709590
-31.620564	-1.468512	1.376320	0.005950	0.709277
-32.346387	-1.347039	1.381325	0.006085	0.709262
-32.855941	-1.258845	1.386330	0.006180	0.709257
-31.885483	-1.426581	1.391334	0.005999	0.709268
-32.055173	-1.398958	1.396339	0.006030	0.709263
-32.712028	-1.283419	1.401344	0.006152	0.709260
-32.267586	-1.360879	1.406349	0.006069	0.709264
-32.417117	-1.422952	1.411354	0.006097	0.709087
-33.518331	-1.292426	1.416358	0.006302	0.708956
-33.237842	-1.346165	1.421363	0.006250	0.708948
-33.287101	-1.335677	1.426368	0.006259	0.708952
-33.285577	-1.332719	1.431373	0.006258	0.708959
-33.561897	-1.288350	1.436378	0.006309	0.708949
-33.108017	-1.364883	1.441382	0.006225	0.708958
-33.073486	-1.381725	1.446387	0.006218	0.708937
-33.876368	-1.389308	1.451392	0.006368	0.708636
-33.829811	-1.396170	1.456397	0.006359	0.708639
-34.288010	-1.318369	1.461402	0.006444	0.708632
-34.023917	-1.360262	1.466406	0.006394	0.708642
-34.139611	-1.342376	1.471411	0.006416	0.708637
-34.361233	-1.302454	1.476416	0.006457	0.708638
-33.970887	-1.369498	1.481421	0.006384	0.708644
-34.641315	-1.384379	1.486426	0.006509	0.708375
-34.969012	-1.340351	1.491430	0.006570	0.708346
-34.915437	-1.351814	1.496435	0.006559	0.708343
-34.967803	-1.341435	1.501440	0.006569	0.708345
-35.060416	-1.321819	1.506445	0.006586	0.708352
-35.166872	-1.307603	1.511450	0.006606	0.708343
-35.000974	-1.334529	1.516454	0.006575	0.708348
-35.108604	-1.420029	1.521459	0.006595	0.708139
-35.995745	-1.327088	1.526464	0.006760	0.708009
-35.782832	-1.363681	1.531469	0.006720	0.708012
-36.103827	-1.309160	1.536474	0.006779	0.708007
-36.009655	-1.323343	1.541478	0.006762	0.708012
-35.467482	-1.421581	1.546483	0.006661	0.708009
-35.836432	-1.355982	1.551488	0.006729	0.708009
-36.136273	-1.400320	1.556493	0.006785	0.707813
-36.775364	-1.347626	1.561498	0.006904	0.707691
-36.649677	-1.365094	1.566502	0.006880	0.707701
-36.575630	-1.380828	1.571507	0.006866	0.707696
-36.873437	-1.328959	1.576512	0.006921	0.707694
-36.654835	-1.364894	1.581517	0.006880	0.707701
-37.128783	-1.286688	1.586522	0.006968	0.707688
-36.847028	-1.416672	1.591526	0.006916	0.707529
-37.681131	-1.346070	1.596531	0.007071	0.707372
-37.470001	-1.384215	1.601536	0.007032	0.707372
-37.383829	-1.395808	1.606541	0.007015	0.707380
-37.890050	-1.310134	1.611546	0.007109	0.707371
-37.534286	-1.369820	1.616550	0.007043	0.707379
-37.776376	-1.327958	1.621555	0.007088	0.707376
-37.921574	-1.369322	1.626560	0.007115	0.707242
-38.523055	-1.341975	1.631565	0.007227	0.707082
-38.393655	-1.368507	1.636570	0.007202	0.707075
-38.579611	-1.329652	1.641574	0.007237	0.707087
-38.316585	-1.380353	1.646579	0.007188	0.707080
-38.503547	-1.347733	1.651584	0.007222	0.707078
-38.446575	-1.355951	1.656589	0.007212	0.707083
-38.785176	-1.382439	1.661594	0.007274	0.706909
-39.606162	-1.313941	1.666598	0.007427	0.706753
-39.284621	-1.371263	1.671603	0.007367	0.706753
-39.548869	-1.326459	1.676608	0.007416	0.706749
-39.483502	-1.335087	1.681613	0.007404	0.706755
-39.445467	-1.345487	1.686618	0.007397	0.706748
-39.410142	-1.348565	1.691622	0.007390	0.706755
-39.401320	-1.385697	1.696627	0.007388	0.706684
-40.447647	-1.319145	1.701632	0.007583	0.706443
-40.442134	-1.317454	1.706637	0.007581	0.706449
-40.724688	-1.271716	1.711642	0.007634	0.706440
-40.242713	-1.354608	1.716646	0.007544	0.706446
-40.385108	-1.331679	1.721651	0.007570	0.706442
-40.723527	-1.272758	1.726656	0.007633	0.706439
-40.166032	-1.369035	1.731661	0.007529	0.706446
-40.685755	-1.392699	1.736666	0.007626	0.706212
-41.836225	-1.228814	1.741670	0.007840	0.706130
-41.045440	-1.371029	1.746675	0.007692	0.706127
-41.341393	-1.318938	1.751680	0.007747	0.706126
-41.601688	-1.270526	1.756685	0.007796	0.706131
-41.331672	-1.323208	1.761690	0.007745	0.706122
-41.145794	-1.354021	1.766694	0.007710	0.706127
-41.289491	-1.375304	1.771699	0.007737	0.706033
-42.255606	-1.289207	1.776704	0.007917	0.705860
-41.611325	-1.400379	1.781709	0.007797	0.705868
-42.233955	-1.293274	1.786714	0.007912	0.705860
-42.089276	-1.316938	1.791718	0.007885	0.705865
-41.771594	-1.374895	1.796723	0.007826	0.705863
-41.929278	-1.348267	1.801728	0.007855	0.705860
-42.286154	-1.409895	1.806733	0.007921	0.705608
-43.024413	-1.319681	1.811738	0.008059	0.705525
-42.872462	-1.343983	1.816742	0.008030	0.705531
-42.908505	-1.340513	1.821747	0.008037	0.705526
-42.933881	-1.334406	1.826752	0.008041	0.705529
-42.561410	-1.399416	1.831757	0.007972	0.705532
-42.964951	-1.336870	1.836762	0.008047	0.705514
-43.753617	-1.343671	1.841766	0.008193	0.705217
-43.574316	-1.376844	1.846771	0.008160	0.705215
-43.886717	-1.323330	1.851776	0.008218	0.705211
-43.902647	-1.316039	1.856781	0.008221	0.705221
-43.748197	-1.349511	1.861786	0.008192	0.705209
-43.711467	-1.351802	1.866790	0.008185	0.705218
-43.800175	-1.347508	1.871795	0.008201	0.705195
-44.614257	-1.356951	1.876800	0.008353	0.704884
-44.545088	-1.364640	1.881805	0.008339	0.704894
-44.973468	-1.292927	1.886810	0.008419	0.704885
-44.756093	-1.328238	1.891814	0.008378	0.704892
-44.668331	-1.343930	1.896819	0.008362	0.704892
-44.834415	-1.317583	1.901824	0.008393	0.704886
-44.862707	-1.311035	1.906829	0.008398	0.704889
-44.964380	-1.409879	1.911834	0.008417	0.704654
-45.569285	-1.333031	1.916838	0.008529	0.704592
-45.419987	-1.361669	1.921843	0.008501	0.704588
-45.360800	-1.373894	1.926848	0.008490	0.704585
-45.535105	-1.337791	1.931853	0.008522	0.704595
-45.612120	-1.328405	1.936858	0.008536	0.704587
-45.643362	-1.326832	1.941862	0.008542	0.704579
-46.174968	-1.391289	1.946867	0.008641	0.704259
-46.343516	-1.361634	1.951872	0.008672	0.704258
-46.772633	-1.282000	1.956877	0.008752	0.704265
-46.661474	-1.305890	1.961882	0.008731	0.704257
-46.312453	-1.364406	1.966886	0.008666	0.704265
-46.590551	-1.317349	1.971891	0.008717	0.704260
-46.654768	-1.307301	1.976896	0.008729	0.704257
-46.574351	-1.437106	1.981901	0.008714	0.704025
-47.433693	-1.323375	1.986906	0.008874	0.703946
-47.561154	-1.297949	1.991910	0.008897	0.703951
-47.093565	-1.380973	1.996915	0.008810	0.703952
-47.619763	-1.288550	2.001920	0.008908	0.703950

-47.521642	-1.307142	2.011917	0.008889	0.703948
-48.090199	-1.302829	2.021914	0.008995	0.703753
-48.183659	-1.346017	2.031910	0.009012	0.703633
-48.396542	-1.307727	2.041907	0.009051	0.703634
-48.415549	-1.304275	2.051904	0.009054	0.703635
-47.847208	-1.303404	2.061901	0.008948	0.703842
-47.948245	-1.247206	2.071898	0.008967	0.703920
-47.507710	-1.311815	2.081894	0.008884	0.703949
-47.355524	-1.338225	2.091891	0.008856	0.703951
-47.378187	-1.334508	2.101888	0.008860	0.703951
-47.626440	-1.291656	2.111885	0.008905	0.703948
-47.608686	-1.294797	2.121882	0.008902	0.703949
-47.390217	-1.334807	2.131878	0.008861	0.703948
-47.453882	-1.322152	2.141875	0.008872	0.703951
-46.959231	-1.320069	2.151872	0.008780	0.704134
-46.705390	-1.305146	2.161869	0.008732	0.704256
-46.681806	-1.310179	2.171866	0.008727	0.704255
-46.547809	-1.333617	2.181862	0.008702	0.704256
-46.677709	-1.310161	2.191859	0.008726	0.704257
-45.710092	-1.319687	2.201856	0.008546	0.704587
-45.653260	-1.328980	2.211853	0.008535	0.704589
-45.740000	-1.315313	2.221850	0.008550	0.704586
-45.766478	-1.309326	2.231846	0.008555	0.704589
-45.124086	-1.305173	2.241843	0.008435	0.704829
-44.971389	-1.303349	2.251840	0.008406	0.704888
-45.144579	-1.273806	2.261837	0.008438	0.704886
-44.800237	-1.313751	2.271834	0.008374	0.704930
-43.997747	-1.316416	2.281830	0.008224	0.705213
-43.872660	-1.337836	2.291827	0.008200	0.705216
-44.058538	-1.305062	2.301824	0.008235	0.705216
-43.931937	-1.260561	2.311821	0.008211	0.705351
-42.797199	-1.374408	2.321818	0.007999	0.705530
-43.220722	-1.298454	2.331814	0.008078	0.705532
-43.065639	-1.326347	2.341811	0.008048	0.705532
-42.267270	-1.349901	2.351808	0.007899	0.705771
-42.193676	-1.315167	2.361805	0.007885	0.705868
-41.938801	-1.363452	2.371802	0.007838	0.705863
-42.139627	-1.327159	2.381798	0.007875	0.705865
-41.610006	-1.311956	2.391795	0.007776	0.706086
-41.445703	-1.318986	2.401792	0.007745	0.706131
-41.440290	-1.321285	2.411789	0.007743	0.706129
-41.049023	-1.318778	2.421786	0.007670	0.706275
-40.492845	-1.332584	2.431782	0.007566	0.706447
-40.511996	-1.330039	2.441779	0.007570	0.706446
-40.371458	-1.354364	2.451776	0.007543	0.706448
-39.817445	-1.311548	2.461773	0.007440	0.706733
-39.506941	-1.359245	2.471770	0.007381	0.706749
-39.564114	-1.348599	2.481766	0.007392	0.706751
-39.249757	-1.343675	2.491763	0.007333	0.706874
-38.684972	-1.340563	2.501760	0.007227	0.707083
-38.800001	-1.323574	2.511757	0.007248	0.707077
-38.813789	-1.320545	2.521754	0.007251	0.707079
-38.057337	-1.313677	2.531750	0.007109	0.707364
-37.815238	-1.349599	2.541747	0.007064	0.707379
-37.966403	-1.322861	2.551744	0.007092	0.707379
-37.783627	-1.268132	2.561741	0.007057	0.707555
-37.123717	-1.314050	2.571738	0.006934	0.707699
-37.274435	-1.286769	2.581734	0.006962	0.707701
-36.837429	-1.319943	2.591731	0.006880	0.707791
-36.325529	-1.300358	2.601728	0.006785	0.708014
-36.164248	-1.330481	2.611725	0.006754	0.708012
-36.385530	-1.291597	2.621722	0.006795	0.708011
-35.638441	-1.268544	2.631718	0.006656	0.708325
-35.274332	-1.320037	2.641715	0.006588	0.708353
-35.505038	-1.279514	2.651712	0.006630	0.708352
-34.987964	-1.299258	2.661709	0.006534	0.708498
-34.520902	-1.312061	2.671706	0.006446	0.708640
-34.416671	-1.330025	2.681702	0.006426	0.708642
-34.446437	-1.319816	2.691699	0.006432	0.708652
-33.882681	-1.266938	2.701696	0.006326	0.708960
-33.530098	-1.330609	2.711693	0.006260	0.708959
-33.776662	-1.287106	2.721690	0.006306	0.708959
-33.210373	-1.296694	2.731686	0.006200	0.709142
-32.624585	-1.339762	2.741683	0.006091	0.709265
-32.742094	-1.320666	2.751680	0.006112	0.709262
-32.685358	-1.320167	2.761677	0.006101	0.709284
-31.947032	-1.297667	2.771674	0.005964	0.709593
-31.670609	-1.346277	2.781670	0.005912	0.709595
-31.849696	-1.314528	2.791667	0.005945	0.709596
-31.620431	-1.279164	2.801664	0.005902	0.709749
-30.923627	-1.331365	2.811661	0.005772	0.709893
-31.082310	-1.303057	2.821658	0.005801	0.709894
-30.828304	-1.340987	2.831654	0.005753	0.709909
-30.223508	-1.292352	2.841651	0.005640	0.710222
-30.086209	-1.318669	2.851648	0.005614	0.710219
-29.939526	-1.344664	2.861645	0.005587	0.710220
-29.923565	-1.269259	2.871642	0.005583	0.710377
-28.804473	-1.391086	2.881638	0.005375	0.710533
-29.288910	-1.302772	2.891635	0.005465	0.710538
-29.210357	-1.317915	2.901632	0.005450	0.710536
-28.529877	-1.282657	2.911629	0.005323	0.710849
-28.462579	-1.283270	2.921626	0.005310	0.710873
-28.184291	-1.333811	2.931622	0.005258	0.710871
-28.047691	-1.295254	2.941619	0.005232	0.710998
-27.510402	-1.320726	2.951616	0.005131	0.711138
-27.660126	-1.293468	2.961613	0.005159	0.711140
-27.604026	-1.284679	2.971610	0.005148	0.711178
-26.560108	-1.334285	2.981606	0.004953	0.711451
-26.667584	-1.313381	2.991603	0.004973	0.711455
-26.690651	-1.308654	3.001600	0.004977	0.711457
-26.176668	-1.288382	3.011597	0.004881	0.711681
-25.849603	-1.306539	3.021594	0.004820	0.711762
-25.544936	-1.359819	3.031590	0.004763	0.711764
-25.701632	-1.301294	3.041587	0.004792	0.711826
-24.870333	-1.315424	3.051584	0.004636	0.712094
-24.711927	-1.344523	3.061581	0.004607	0.712093
-24.831649	-1.324886	3.071578	0.004629	0.712090
-24.547181	-1.286831	3.081574	0.004575	0.712267
-24.078028	-1.307907	3.091571	0.004488	0.712393
-23.994058	-1.323232	3.101568	0.004472	0.712392
-23.991816	-1.290685	3.111565	0.004471	0.712459
-23.234021	-1.300379	3.121562	0.004329	0.712709
-23.104425	-1.323480	3.131558	0.004305	0.712710
-23.205909	-1.304073	3.141555	0.004323	0.712713
-22.394883	-1.324850	3.151552	0.004172	0.712960
-22.166918	-1.334497	3.161549	0.004129	0.713022
-22.258812	-1.318565	3.171546	0.004146	0.713022
-22.215095	-1.290196	3.181542	0.004138	0.713095
-21.202665	-1.338417	3.191539	0.003949	0.713358
-21.084792	-1.359231	3.201536	0.003927	0.713359
-21.360704	-1.311534	3.211533	0.003978	0.713357
-21.165039	-1.270534	3.221530	0.003941	0.713508
-20.334262	-1.347192	3.231526	0.003786	0.713651
-20.589048	-1.299920	3.241523	0.003833	0.713655
-20.405529	-1.314860	3.251520	0.003798	0.713691
-19.635494	-1.312535	3.261517	0.003655	0.713969
-19.232046	-1.385053	3.271514	0.003579	0.713969
-19.664722	-1.307660	3.281510	0.003659	0.713970
-19.232395	-1.309226	3.291507	0.003579	0.714120
-18.328684	-1.390899	3.301504	0.003410	0.714279
-18.682441	-1.328551	3.311501	0.003475	0.714278
-18.579737	-1.348353	3.321498	0.003456	0.714276
-17.881399	-1.330492	3.331494	0.003326	0.714559
-17.703522	-1.333616	3.341491	0.003292	0.714616
-17.619216	-1.349274	3.351488	0.003276	0.714616
-17.759799	-1.295346	3.361485	0.003302	0.714674
-16.607343	-1.382951	3.371482	0.003087	0.714908
-16.722047	-1.362840	3.381478	0.003108	0.714908
-16.783640	-1.350615	3.391475	0.003119	0.714911
-16.330696	-1.338570	3.401472	0.003035	0.715096
-15.848969	-1.356053	3.411469	0.002945	0.715232
-15.884980	-1.351340	3.421466	0.002951	0.715229
-15.806896	-1.363053	3.431462	0.002936	0.715234
-15.101567	-1.343547	3.441459	0.002804	0.715523
-14.741403	-1.394001	3.451456	0.002737	0.715551
-15.040085	-1.343244	3.461453	0.002792	0.715546
-14.734690	-1.367504	3.471450	0.002735	0.715607
-14.001163	-1.361180	3.481446	0.002598	0.715879
-13.903327	-1.377197	3.491443	0.002580	0.715882
-13.740652	-1.406184	3.501440	0.002549	0.715883
-13.862841	-1.329766	3.511437	0.002571	0.715992
-12.812037	-1.448290	3.521434	0.002375	0.716129
-13.328953	-1.355546	3.531430	0.002471	0.716131
-13.031446	-1.407367	3.541427	0.002416	0.716134
-12.479267	-1.367128	3.551424	0.002312	0.716409
-12.209334	-1.396001	3.561421	0.002262	0.716447
-12.006667	-1.434793	3.571418	0.002224	0.716443
-12.141314	-1.372572	3.581414	0.002248	0.716519
-11.158984	-1.429091	3.591411	0.002065	0.716754
-11.178322	-1.424509	3.601408	0.002068	0.716757
-11.258606	-1.412229	3.611405	0.002083	0.716754
-10.841304	-1.389978	3.621402	0.002005	0.716946
-10.320910	-1.414111	3.631398	0.001908	0.717082
-10.125619	-1.446455	3.641395	0.001871	0.717087
-10.246482	-1.426001	3.651392	0.001893	0.717086
-9.721409	-1.397133	3.661389	0.001795	0.717329
-9.381099	-1.432109	3.671386	0.001731	0.717380
-9.399227	-1.429796	3.681382	0.001734	0.717379
-9.157708	-1.446620	3.691379	0.001689	0.717431
-8.573104	-1.412753	3.701376	0.001580	0.717705
-8.223620	-1.475642	3.711373	0.001515	0.717704
-8.338726	-1.456609	3.721370	0.001536	0.717702
-8.265511	-1.417778	3.731366	0.001522	0.717805
-7.328849	-1.477118	3.741363	0.001347	0.718018
-7.506679	-1.445452	3.751360	0.001380	0.718019
-7.331016	-1.477656	3.761357	0.001347	0.718017
-7.080177	-1.417419	3.771354	0.001300	0.718225
-6.354099	-1.484815	3.781350	0.001164	0.718348
-6.122591	-1.523483	3.791347	0.001121	0.718354
-6.213614	-1.507278	3.801344	0.001137	0.718354
-5.733650	-1.520574	3.811341	0.001048	0.718498
-5.381226	-1.508683	3.821338	0.000982	0.718646
-5.208270	-1.541315	3.831334	0.000949	0.718643
-4.956922	-1.585019	3.841331	0.000902	0.718645
-5.209441	-1.495426	3.851328	0.000949	0.718734
-4.283865	-1.544433	3.861325	0.000776	0.718963
-4.366855	-1.531481	3.871322	0.000791	0.718960
-4.179178	-1.564992	3.881318	0.000756	0.718961
-4.230083	-1.491240	3.891315	0.000765	0.719089
-3.508967	-1.527469	3.901312	0.000630	0.719272
-3.480282	-1.532425	3.911309	0.000625	0.719273
-3.593507	-1.513891	3.921306	0.000645	0.719270
-2.913516	-1.500431	3.931302	0.000518	0.719536
-2.622671	-1.517425	3.941299	0.000464	0.719605
-2.711762	-1.501643	3.951296	0.000480	0.719606
-2.812223	-1.440856	3.961293	0.000499	0.719691
-2.185847	-1.445212	3.971290	0.000382	0.719903
-2.215779	-1.440125	3.981286	0.000387	0.719903
-1.959189	-1.458179	3.991283	0.000339	0.719958
-1.488979	-1.404958	4.001280	0.000251	0.720228
-1.650762	-1.378573	4.011277	0.000281	0.720224
-1.549215	-1.362414	4.021274	0.000261	0.720292
-1.354932	-1.273170	4.031270	0.000225	0.720537
-1.230305	-1.292749	4.041267	0.000201	0.720542
-1.038280	-1.212351	4.051264	0.000165	0.720769
-1.011934	-1.161761	4.061261	0.000160	0.720878
-1.038826	-1.108555	4.071258	0.000164	0.720974
-0.737086	-1.086844	4.081254	0.000108	0.721123
-0.761769	-1.035207	4.091251	0.000112	0.721216
-0.919485	-0.894090	4.101248	0.000141	0.721439
-0.699531	-0.863173	4.111245	0.000100	0.721578
-0.637731	-0.791035	4.121242	0.000088	0.721742
-0.585640	-0.677211	4.131238	0.000078	0.721984
-0.507567	-0.626784	4.141235	0.000063	0.722111
-0.405000	-0.512807	4.151232	0.000043	0.722372
-0.294045	-0.435514	4.161229	0.000022	0.722563
-0.400633	-0.324239	4.171226	0.000042	0.722745
-0.354295	-0.202205	4.181222	0.000033	0.723001
-0.055415	-0.114449	4.191219	-0.000023	0.723278
-0.218748	0.019379	4.201216	0.000007	0.723484
-0.020045	0.095637	4.211213	-0.000031	0.723703
0.000000	0.282051	4.221210	-0.000035	0.724076

0.021894	0.915457	4.226214	-0.000040	0.725324
0.109004	2.156305	4.231219	-0.000057	0.727777
0.451702	3.959515	4.236224	-0.000122	0.731401
0.879777	6.296010	4.241229	-0.000203	0.736065
1.395125	9.128393	4.246234	-0.000301	0.741677
1.607411	12.505311	4.251238	-0.000343	0.748179
2.235713	16.259576	4.256243	-0.000463	0.755471
3.045472	20.385678	4.261248	-0.000617	0.763445
3.660758	24.968558	4.266253	-0.000734	0.772112
4.157729	29.924633	4.271258	-0.000830	0.781322
4.847806	35.206622	4.276262	-0.000962	0.791071
5.309539	40.841412	4.281267	-0.001052	0.801253
5.689381	46.791941	4.286272	-0.001127	0.811834
6.479215	52.959334	4.291277	-0.001278	0.822777
7.134747	59.426034	4.296282	-0.001405	0.834045
7.418238	66.169993	4.301286	-0.001462	0.845517
7.909224	73.105367	4.306291	-0.001558	0.857213
8.347335	80.244942	4.311296	-0.001644	0.869069
9.060215	87.535087	4.316301	-0.001782	0.881085
9.581914	95.025820	4.321306	-0.001884	0.893205
10.189969	102.661500	4.326310	-0.002003	0.905412
10.779982	110.458726	4.331315	-0.002118	0.917702
11.335004	118.357778	4.336320	-0.002226	0.929975
11.997494	126.366478	4.341325	-0.002355	0.942280
12.674841	134.466260	4.346330	-0.002487	0.954566
13.215183	142.669075	4.351334	-0.002593	0.966811
13.918584	150.936355	4.356339	-0.002729	0.979038
14.642495	159.283316	4.361344	-0.002870	0.991232
16.025069	167.569088	4.366349	-0.003133	1.003353
16.504813	176.060638	4.371354	-0.003228	1.015397
17.170511	184.558138	4.376358	-0.003358	1.027352
17.878636	193.096178	4.381363	-0.003495	1.039235
18.518277	201.654376	4.386368	-0.003620	1.050993
19.380233	210.220234	4.391373	-0.003786	1.062683
20.158020	218.823819	4.396378	-0.003937	1.074276
20.799787	227.440732	4.401382	-0.004062	1.085732
21.457870	236.082632	4.406387	-0.004190	1.097103
22.075840	244.725784	4.411392	-0.004311	1.108350
23.012919	253.331057	4.416397	-0.004492	1.119505
23.476671	262.007158	4.421402	-0.004584	1.130537
24.316173	270.619677	4.426406	-0.004746	1.141463
24.917612	279.311158	4.431411	-0.004864	1.152331
25.323261	287.966140	4.436416	-0.004945	1.163013
26.272105	296.529861	4.441421	-0.005127	1.173599
27.043604	305.105303	4.446426	-0.005277	1.184068
27.645677	313.725175	4.451430	-0.005395	1.194462
28.292649	322.306362	4.456435	-0.005521	1.204731
28.901583	330.885661	4.461440	-0.005640	1.214902
29.628404	339.444345	4.466445	-0.005781	1.224989
30.021128	348.058038	4.471450	-0.005860	1.234990
30.657018	356.583868	4.476454	-0.005984	1.244858
31.362527	365.109764	4.481459	-0.006121	1.254661
31.637943	373.664241	4.486464	-0.006178	1.264339
32.130846	382.197302	4.491469	-0.006276	1.273959
32.614417	390.680825	4.496474	-0.006372	1.283451
32.934751	399.206832	4.501478	-0.006437	1.292890
33.519839	407.660616	4.506483	-0.006552	1.302230
33.998976	416.194506	4.511488	-0.006646	1.311570
34.648719	424.658479	4.516493	-0.006773	1.320800
35.173154	433.060108	4.521498	-0.006876	1.329877
35.782387	441.457838	4.526502	-0.006996	1.338903
36.543398	449.827976	4.531507	-0.007143	1.347865
36.878432	458.260661	4.536512	-0.007211	1.356760
37.419292	466.632731	4.541517	-0.007317	1.365569
38.387849	474.951668	4.546522	-0.007503	1.374339
38.897410	483.315821	4.551526	-0.007604	1.383022
39.240900	491.730466	4.556531	-0.007673	1.391674
39.556971	500.105603	4.561536	-0.007738	1.400228
39.966890	508.461412	4.566541	-0.007820	1.408726
40.633655	516.769042	4.571546	-0.007949	1.417166
41.099343	525.094027	4.576550	-0.008042	1.425541
41.659292	533.435313	4.581555	-0.008152	1.433899
41.963670	541.760362	4.586560	-0.008214	1.442150
42.361970	550.090975	4.591565	-0.008294	1.450375
42.848981	558.397872	4.596570	-0.008390	1.458544
43.519159	566.654133	4.601574	-0.008520	1.466648
44.050692	575.008373	4.606579	-0.008625	1.474779
44.366904	583.297565	4.611584	-0.008689	1.482770
44.659848	591.598813	4.616589	-0.008749	1.490725
45.104148	599.861182	4.621594	-0.008838	1.498625
45.540736	608.118918	4.626598	-0.008925	1.506478
45.787780	616.432579	4.631603	-0.008976	1.514313
46.322622	624.647228	4.636608	-0.009081	1.522059
46.774683	632.906795	4.641613	-0.009171	1.529795
47.216825	641.164837	4.646618	-0.009259	1.537489
47.772186	649.381447	4.651622	-0.009368	1.545123
48.191005	657.670969	4.656627	-0.009451	1.552766
48.343989	665.919392	4.661632	-0.009485	1.560295
48.969136	674.122966	4.666637	-0.009607	1.567816
49.569135	682.333298	4.671642	-0.009725	1.575303
50.043650	690.555196	4.676646	-0.009818	1.582747
50.580725	698.771646	4.681651	-0.009924	1.590160
50.761096	707.038172	4.686656	-0.009963	1.597532
51.206299	715.245612	4.691661	-0.010051	1.604855
51.649510	723.459979	4.696666	-0.010140	1.612151
52.020205	731.673936	4.701670	-0.010214	1.619403
52.626458	739.858277	4.706675	-0.010332	1.626630
52.719597	748.172727	4.711680	-0.010355	1.633867
53.041275	756.359486	4.716685	-0.010421	1.640992
53.346644	764.540150	4.721690	-0.010483	1.648080
53.829137	772.721281	4.726694	-0.010578	1.655161
54.378722	780.889248	4.731699	-0.010686	1.662210
54.649138	789.083138	4.736704	-0.010742	1.669213
54.963599	797.301651	4.741709	-0.010806	1.676214
55.403826	805.457249	4.746714	-0.010894	1.683149
55.646413	813.648272	4.751718	-0.010944	1.690059
56.150184	821.829045	4.756723	-0.011044	1.696967
56.463701	829.999187	4.761728	-0.011108	1.703812
56.973065	838.167165	4.766733	-0.011208	1.710654
57.074669	846.403068	4.771738	-0.011232	1.717472
57.421512	854.548331	4.776742	-0.011302	1.724220
57.944036	862.695068	4.781747	-0.011405	1.730965
58.019676	870.894047	4.786752	-0.011425	1.737670
58.531424	879.026317	4.791757	-0.011526	1.744349
58.814428	887.199647	4.796762	-0.011584	1.751008
59.220107	895.352112	4.801766	-0.011665	1.757640
59.678821	903.494472	4.806771	-0.011756	1.764245
59.929721	911.670936	4.811776	-0.011808	1.770827
60.533401	919.812034	4.816781	-0.011926	1.777400
60.744038	927.983821	4.821786	-0.011970	1.783924
61.217617	936.143567	4.826790	-0.012064	1.790447
61.502032	944.351799	4.831795	-0.012123	1.796962
61.699272	952.481352	4.836800	-0.012165	1.803380
61.996681	960.629588	4.841805	-0.012226	1.809803
62.314949	968.784040	4.846810	-0.012290	1.816210
62.747100	976.888166	4.851814	-0.012376	1.822569
63.313588	985.004171	4.856819	-0.012487	1.828930
63.672393	993.135624	4.861824	-0.012560	1.835257
63.961715	1001.281611	4.866829	-0.012619	1.841565
64.293527	1009.423231	4.871834	-0.012686	1.847853
64.432270	1017.594707	4.876838	-0.012717	1.854120
65.062783	1025.685285	4.881843	-0.012840	1.860361
65.439145	1033.802562	4.886848	-0.012916	1.866573
65.450951	1042.026440	4.891853	-0.012924	1.872801
65.757465	1050.152009	4.896858	-0.012986	1.878969
66.201708	1058.218346	4.901862	-0.013074	1.885088
66.603589	1066.359254	4.906867	-0.013155	1.891238
66.742179	1074.510969	4.911872	-0.013186	1.897347
67.083978	1082.624701	4.916877	-0.013255	1.903430
67.410409	1090.755888	4.921882	-0.013321	1.909505
67.735435	1098.882447	4.926886	-0.013387	1.915557
68.039222	1106.999452	4.931891	-0.013449	1.921580
68.276360	1115.112740	4.936896	-0.013499	1.927575
68.727128	1123.238725	4.941901	-0.013588	1.933583
68.994610	1131.359385	4.946906	-0.013643	1.939549
69.292646	1139.461667	4.951910	-0.013704	1.945486
69.834376	1147.594578	4.956915	-0.013811	1.951455
69.820026	1155.770617	4.961920	-0.013814	1.957375
70.288495	1163.824237	4.966925	-0.013906	1.963242
70.532292	1171.943554	4.971930	-0.013957	1.969114
70.672573	1180.062939	4.976934	-0.013989	1.974957
71.127616	1188.146251	4.981939	-0.014079	1.980791
71.563503	1196.225542	4.986944	-0.014165	1.986603
71.813999	1204.369632	4.991949	-0.014218	1.992424
72.246203	1212.458557	4.996954	-0.014303	1.998208
72.676011	1220.530550	5.001958	-0.014389	2.003963
73.100912	1228.642141	5.006963	-0.014473	2.009729
73.159401	1236.788039	5.011968	-0.014490	2.015464
73.368691	1244.899266	5.016973	-0.014534	2.021175
73.676077	1252.994563	5.021978	-0.014597	2.026868
73.951178	1261.135580	5.026982	-0.014654	2.032573
74.281418	1269.250691	5.031987	-0.014721	2.038251
74.741362	1277.288733	5.036992	-0.014812	2.043872
75.055581	1285.396669	5.041997	-0.014876	2.049511
75.377328	1293.498225	5.047002	-0.014941	2.055131
75.658347	1301.589558	5.052006	-0.014999	2.060724
75.898273	1309.705477	5.057011	-0.015049	2.066315
76.055803	1317.817910	5.062016	-0.015084	2.071880
76.219580	1325.942452	5.067021	-0.015120	2.077439
76.548917	1334.003003	5.072026	-0.015186	2.082956
76.914225	1342.080432	5.077030	-0.015260	2.088474
77.210329	1350.191882	5.082035	-0.015320	2.093993
77.432548	1358.280812	5.087040	-0.015367	2.099474
77.864954	1366.343924	5.092045	-0.015453	2.104945
78.049043	1374.484521	5.097050	-0.015493	2.110429
78.504064	1382.590763	5.102054	-0.015583	2.115903
79.274119	1390.607652	5.107059	-0.015732	2.121332
79.353238	1398.709059	5.112064	-0.015752	2.126738
79.513814	1406.832845	5.117069	-0.015787	2.132152
79.958547	1414.905256	5.122074	-0.015876	2.137546
80.186766	1422.984314	5.127078	-0.015924	2.142910
80.387279	1431.095828	5.132083	-0.015966	2.148279
80.853816	1439.164100	5.137088	-0.016059	2.153632
81.104522	1447.255773	5.142093	-0.016111	2.158966
81.383441	1455.312787	5.147098	-0.016168	2.164266
81.487423	1463.432405	5.152102	-0.016193	2.169579
81.848315	1471.532836	5.157107	-0.016266	2.174890
82.000516	1479.609161	5.162112	-0.016299	2.180152
82.184701	1487.709513	5.167117	-0.016339	2.185421
82.476633	1495.800285	5.172122	-0.016399	2.190680
82.700090	1503.898131	5.177126	-0.016446	2.195925
83.024490	1511.964352	5.182131	-0.016512	2.201147
83.257005	1520.013773	5.187136	-0.016561	2.206337
83.562139	1528.099426	5.192141	-0.016623	2.211544
83.789962	1536.190794	5.197146	-0.016671	2.216736
83.819233	1544.280425	5.202150	-0.016682	2.221896
84.349174	1552.332916	5.207155	-0.016786	2.227066
84.660727	1560.403586	5.212160	-0.016849	2.232216
84.665945	1568.533516	5.217165	-0.016856	2.237364
84.940435	1576.581490	5.222170	-0.016912	2.242472
85.081849	1584.657911	5.227174	-0.016944	2.247575
85.526642	1592.750303	5.232179	-0.017032	2.252703
85.772042	1600.806755	5.237184	-0.017083	2.257780
86.155574	1608.866582	5.242189	-0.017160	2.262858
86.453391	1616.946932	5.247194	-0.017221	2.267931
86.717583	1625.109437	5.252198	-0.017276	2.273041
86.924030	1633.194697	5.257203	-0.017319	2.278086
87.136960	1641.212761	5.262208	-0.017365	2.283079
87.320844	1649.269710	5.267213	-0.017404	2.288082
87.715308	1657.331118	5.272218	-0.017483	2.293095
87.892898	1665.397433	5.277222	-0.017522	2.298082
88.154937	1673.467774	5.282227	-0.017576	2.303068
88.170844	1681.541679	5.287232	-0.017584	2.308024
88.639406	1689.607975	5.292237	-0.017677	2.313003
88.872148	1697.672831	5.297242	-0.017726	2.317950
88.859797	1705.743965	5.302246	-0.017729	2.322870
89.484808	1713.774839	5.307251	-0.017850	2.327809
89.445743	1721.880945	5.312256	-0.017849	2.332727
89.753356	1729.952622	5.317261	-0.017911	2.337643
89.908436	1738.022417	5.322266	-0.017946	2.342535
90.258696	1746.065123	5.327270	-0.018016	2.347416
90.527182	1754.180011	5.332275	-0.018072	2.352323
90.602169	1762.247429	5.337280	-0.018091	2.357176
90.953895	1770.282970	5.342285	-0.018162	2.362023
91.302304	1778.338322	5.347290	-0.018232	2.366871
91.367679	1786.434923	5.352294	-0.018250	2.371711
91.655726	1794.509275	5.357299	-0.018309	2.376545
91.871862	1802.550539	5.362304	-0.018355	2.381345
92.253613	1810.602835	5.367309	-0.018431	2.386154
92.354544	1818.699724	5.372314	-0.018455	2.390958
92.528311	1826.776807	5.377318	-0.018493	2.395746
93.076159	1834.802779	5.382323	-0.018601	2.400523
93.150376	1842.856195	5.387328	-0.018620	2.405271
93.287118	1850.942528	5.392333	-0.018651	2.410033
93.623476	1859.025898	5.397338	-0.018719	2.414799
93.716389	1867.078468	5.402342	-0.018742	2.419519
94.150329	1875.128148	5.407347	-0.018828	2.424254
94.252340	1883.201039	5.412352	-0.018852	2.428968
94.637590	1891.321844	5.417357	-0.018929	2.433723
94.935370	1899.354888	5.422362	-0.018990	2.438410
95.245968	1907.363353	5.427366	-0.019053	2.443076
95.506189	1915.438528	5.432371	-0.019107	2.447767
95.492232	1923.517465	5.437376	-0.019110	2.452430
95.844217	1931.555948	5.442381	-0.019181	2.457089
96.283966	1939.590830	5.447386	-0.019268	2.461743
96.050097	1947.683522	5.452390	-0.019230	2.466371
96.325885	1955.766761	5.457395	-0.019287	2.471024
96.687890	1963.794082	5.462400	-0.019360	2.475642
97.071036	1971.844282	5.467405	-0.019437	2.480265
97.203317	1979.895456	5.472410	-0.019467	2.484863
97.436979	1987.942713	5.477414	-0.019516	2.489456
97.635935	1996.049949	5.482419	-0.019558	2.494073
97.772012	2004.092234	5.487424	-0.019589	2.498640
97.978911	2012.136315	5.492429	-0.019633	2.503205
98.437211	2020.179688	5.497434	-0.019724	2.507779
98.568277	2028.282391	5.502438	-0.019753	2.512354
98.718123	2036.367265	5.507443	-0.019787	2.516913
98.969310	2044.372080	5.512448	-0.019839	2.521425
98.967290	2052.447825	5.517453	-0.019844	2.525951
99.303534	2060.486960	5.522458	-0.019912	2.530473
99.373753	2068.571323	5.527462	-0.019930	2.534993
99.623721	2076.628740	5.532467	-0.019982	2.539502
99.828670	2084.646010	5.537472	-0.020026	2.543978
99.912271	2092.709282	5.542477	-0.020047	2.548463
100.346863	2100.761409	5.547482	-0.020133	2.552958
100.363023	2108.819244	5.552486	-0.020142	2.557420
100.539393	2116.882198	5.557491	-0.020180	2.561887
100.765258	2124.915415	5.562496	-0.020227	2.566334
101.028505	2132.971899	5.567501	-0.020282	2.570789
101.072370	2141.067045	5.572506	-0.020296	2.575241
101.254555	2149.079681	5.577510	-0.020335	2.579651
101.778412	2157.104012	5.582515	-0.020438	2.584083
102.014068	2165.161450	5.587520	-0.020487	2.588505
102.104813	2173.393781	5.592525	-0.020510	2.593005
102.361663	2181.436512	5.597530	-0.020563	2.597405
102.285427	2189.447614	5.602534	-0.020554	2.601759
102.527666	2197.460303	5.607539	-0.020604	2.606127
102.698272	2205.473030	5.612544	-0.020642	2.610483
102.899196	2213.532429	5.617549	-0.020684	2.614859
102.907672	2221.581053	5.622554	-0.020691	2.619209
103.240414	2229.589586	5.627558	-0.020759	2.623552
103.469350	2237.656922	5.632563	-0.020807	2.627912
103.546026	2245.713310	5.637568	-0.020827	2.632250
103.817531	2253.753202	5.642573	-0.020882	2.636584
104.140928	2261.774452	5.647578	-0.020948	2.640904
104.218491	2269.809466	5.652582	-0.020968	2.645208
104.659570	2277.840513	5.657587	-0.021055	2.649527
104.564893	2285.961402	5.662592	-0.021043	2.653852
104.853749	2293.980218	5.667597	-0.021102	2.658140
105.080159	2302.026252	5.672602	-0.021150	2.662432
105.282958	2310.058853	5.677606	-0.021193	2.666708
105.635206	2318.138178	5.682611	-0.021264	2.671012
105.546833	2326.229956	5.687616	-0.021253	2.675287
105.913457	2334.206665	5.692621	-0.021327	2.679523
106.300988	2342.242868	5.697626	-0.021404	2.683786
106.431739	2350.274472	5.702630	-0.021434	2.688023
106.605931	2358.376000	5.707635	-0.021472	2.692292
106.739524	2366.411450	5.712640	-0.021502	2.696518
106.908296	2374.459530	5.717645	-0.021539	2.700746
107.102265	2382.494606	5.722650	-0.021581	2.704962
107.276432	2390.532153	5.727654	-0.021619	2.709171
107.679989	2398.603961	5.732659	-0.021699	2.713406
107.809575	2406.642779	5.737664	-0.021729	2.717600
108.091741	2414.662663	5.742669	-0.021787	2.721787
108.445430	2422.723258	5.747674	-0.021858	2.725994
108.268066	2430.780134	5.752678	-0.021830	2.730159
108.566475	2438.859715	5.757683	-0.021891	2.734359
108.834656	2446.889576	5.762688	-0.021947	2.738524
109.060944	2454.901055	5.767693	-0.021994	2.742672
109.152862	2462.975859	5.772698	-0.022017	2.746837
109.376386	2471.032265	5.777702	-0.022064	2.750994
109.792765	2479.157357	5.782707	-0.022147	2.755193
109.939413	2487.141597	5.787712	-0.022179	2.759296
109.800157	2495.197622	5.792717	-0.022159	2.763413
109.827107	2503.252828	5.797722	-0.022169	2.767533
110.167189	2511.260156	5.802726	-0.022238	2.771641
110.358273	2519.322104	5.807731	-0.022279	2.775762
110.414338	2527.329648	5.812736	-0.022295	2.779841
110.480227	2535.382273	5.817741	-0.022313	2.783938
110.584712	2543.433084	5.822746	-0.022337	2.788030
110.823162	2551.454347	5.827750	-0.022387	2.792109
111.113901	2559.520938	5.832755	-0.022447	2.796208
111.279868	2567.524928	5.837760	-0.022483	2.800262
111.492655	2575.535211	5.842765	-0.022528	2.804315
111.699114	2583.601972	5.847770	-0.022572	2.808392
112.252373	2591.612714	5.852774	-0.022680	2.812454
112.412964	2599.692910	5.857779	-0.022716	2.816522
112.416620	2607.741225	5.862784	-0.022722	2.820559
112.685167	2615.748920	5.867789	-0.022777	2.824586
112.803144	2623.822263	5.872794	-0.022805	2.828631
112.820126	2631.906876	5.877798	-0.022813	2.832669
113.156895	2639.951581	5.882803	-0.022881	2.836701
113.410240	2647.942134	5.887808	-0.022934	2.840695
113.558047	2655.962345	5.892813	-0.022967	2.844692
113.844996	2664.019045	5.897818	-0.023026	2.848709
114.190673	2672.044731	5.902822	-0.023095	2.852709
114.333482	2680.111732	5.907827	-0.023127	2.856712
114.537016	2688.142224	5.912832	-0.023171	2.860695
114.767280	2696.144326	5.917837	-0.023219	2.864659
114.969786	2704.213981	5.922842	-0.023262	2.868650
115.175118	2712.247096	5.927846	-0.023306	2.872618
115.264433	2720.346991	5.932851	-0.023328	2.876606
115.270999	2728.365013	5.937856	-0.023334	2.880544
115.400480	2736.377756	5.942861	-0.023364	2.884481
115.803998	2744.423306	5.947866	-0.023444	2.888443
115.965074	2752.462375	5.952870	-0.023480	2.892384
116.278552	2760.525650	5.957875	-0.023544	2.896339
116.126686	2768.595322	5.962880	-0.023521	2.900267
116.404076	2776.595027	5.967885	-0.023578	2.904179
116.682725	2784.650493	5.972890	-0.023635	2.908112
116.746611	2792.740052	5.977894	-0.023652	2.912045
117.008454	2800.810439	5.982899	-0.023707	2.915974
117.248107	2808.768548	5.987904	-0.023757	2.919842
117.161299	2816.791217	5.992909	-0.023746	2.923719
117.389403	2824.815248	5.997914	-0.023794	2.927608
117.572077	2832.836267	6.002918	-0.023833	2.931488
117.856361	2840.917229	6.007923	-0.023892	2.935397
117.825526	2848.928524	6.012928	-0.023891	2.939251
117.978246	2856.959629	6.017933	-0.023925	2.943119
118.514881	2864.985781	6.022938	-0.024030	2.946999
118.487908	2873.038860	6.027942	-0.024031	2.950858
118.607331	2881.121891	6.032947	-0.024058	2.954734
118.733972	2889.122691	6.037952	-0.024087	2.958565
118.901491	2897.147202	6.042957	-0.024124	2.962406
118.942009	2905.203080	6.047962	-0.024137	2.966249
119.368123	2913.203788	6.052966	-0.024222	2.970081
119.533237	2921.290311	6.057971	-0.024258	2.973935
119.512386	2929.293519	6.062976	-0.024259	2.977736
119.745360	2937.325958	6.067981	-0.024308	2.981558
119.987796	2945.368487	6.072986	-0.024359	2.985381
119.998755	2953.415041	6.077990	-0.024366	2.989189
120.191470	2961.508770	6.082995	-0.024407	2.993023
120.371703	2969.523626	6.088000	-0.024446	2.996815
120.526168	2977.520309	6.093005	-0.024481	3.000592
120.768838	2985.533109	6.098010	-0.024531	3.004376
120.669403	2993.585544	6.103014	-0.024518	3.008157
120.857472	3001.644443	6.108019	-0.024558	3.011950
121.021045	3009.684872	6.113024	-0.024594	3.015729
121.236527	3017.677351	6.118029	-0.024640	3.019484
121.631116	3025.710582	6.123034	-0.024719	3.023261
121.487833	3033.760740	6.128038	-0.024697	3.027015
121.691666	3041.836877	6.133043	-0.024741	3.030794
121.771900	3049.877744	6.138048	-0.024761	3.034545
122.084332	3057.884374	6.143053	-0.024825	3.038287
122.156222	3065.917903	6.148058	-0.024844	3.042025
122.239475	3073.934617	6.153062	-0.024864	3.045752
122.390256	3082.006772	6.158067	-0.024898	3.049503
122.657089	3090.039900	6.163072	-0.024953	3.053236
122.872656	3098.045736	6.168077	-0.024999	3.056950
123.033847	3106.096756	6.173082	-0.025034	3.060678
123.137935	3114.077562	6.178086	-0.025059	3.064366
123.166519	3122.167257	6.183091	-0.025069	3.068096
123.310267	3130.254390	6.188096	-0.025102	3.071826
123.557723	3138.314374	6.193101	-0.025153	3.075544
123.572643	3146.329660	6.198106	-0.025161	3.079225
123.847675	3154.277086	6.203110	-0.025218	3.082884
124.097015	3162.326703	6.208115	-0.025270	3.086583
123.997839	3170.376284	6.213120	-0.025257	3.090262
124.282997	3178.402111	6.218125	-0.025315	3.093944
124.629962	3186.422530	6.223130	-0.025385	3.097621
124.754218	3194.438735	6.228134	-0.025414	3.101282
124.811478	3202.490408	6.233139	-0.025430	3.104952
124.958466	3210.519998	6.238144	-0.025463	3.108611
125.136438	3218.559474	6.243149	-0.025501	3.112272
125.108927	3226.661356	6.248154	-0.025501	3.115947
125.284480	3234.609933	6.253158	-0.025540	3.119558
125.748010	3242.620627	6.258163	-0.025631	3.123206
125.681258	3250.699022	6.263168	-0.025624	3.126856
125.777446	3258.721607	6.268173	-0.025648	3.130484
126.088635	3266.761406	6.273178	-0.025711	3.134125
126.264336	3274.787332	6.278182	-0.025749	3.137750
126.502809	3282.812991	6.283187	-0.025799	3.141373
126.803031	3290.812799	6.288192	-0.025860	3.144983
126.913671	3298.867658	6.293197	-0.025886	3.148605
127.087795	3306.951417	6.298202	-0.025924	3.152239
127.178302	3315.002557	6.303206	-0.025946	3.155850
127.440834	3322.988286	6.308211	-0.026000	3.159435
127.565001	3330.984792	6.313216	-0.026029	3.163015
127.632818	3339.021776	6.318221	-0.026047	3.166607
127.997319	3347.054618	6.323226	-0.026120	3.170205
128.176070	3355.103501	6.328230	-0.026159	3.173799
128.255011	3363.147358	6.333235	-0.026179	3.177382
128.378090	3371.170090	6.338240	-0.026207	3.180953
128.688780	3379.154343	6.343245	-0.026271	3.184511
128.837666	3387.232925	6.348250	-0.026304	3.188100
128.817106	3395.284008	6.353254	-0.026305	3.191666
128.998316	3403.334013	6.358259	-0.026345	3.195235
129.181698	3411.328598	6.363264	-0.026384	3.198777
129.418507	3419.320694	6.368269	-0.026434	3.202315
129.596470	3427.374085	6.373274	-0.026472	3.205874
129.753337	3435.391717	6.378278	-0.026507	3.209413
129.896269	3443.457222	6.383283	-0.026539	3.212968
130.011222	3451.530112	6.388288	-0.026566	3.216521
130.202836	3459.504465	6.393293	-0.026607	3.220030
130.304323	3467.532403	6.398298	-0.026631	3.223555
130.410762	3475.560166	6.403302	-0.026656	3.227076
130.896892	3483.603375	6.408307	-0.026752	3.230616
131.010946	3491.697512	6.413312	-0.026779	3.234159
130.926232	3499.716791	6.418317	-0.026768	3.237657
131.130398	3507.731480	6.423322	-0.026812	3.241161
131.317703	3515.690555	6.428326	-0.026852	3.244637
131.623695	3523.736994	6.433331	-0.026914	3.248151
131.685770	3531.760219	6.438336	-0.026931	3.251642
132.024331	3539.805472	6.443341	-0.027000	3.255150
132.054261	3547.858427	6.448346	-0.027011	3.258644
131.973662	3555.866036	6.453350	-0.027001	3.262111
132.340187	3563.904701	6.458355	-0.027075	3.265606
132.462551	3571.929679	6.463360	-0.027103	3.269081
132.708096	3579.970837	6.468365	-0.027154	3.272564
132.938911	3588.024925	6.473370	-0.027203	3.276049
133.115739	3595.994776	6.478374	-0.027241	3.279491
133.113954	3604.037150	6.483379	-0.027246	3.282954
133.200807	3612.077106	6.488384	-0.027267	3.286415
133.345387	3620.105843	6.493389	-0.027300	3.289871
133.655073	3628.178456	6.498394	-0.027363	3.293348
133.462473	3636.205782	6.503398	-0.027332	3.296782
133.754134	3644.203838	6.508403	-0.027392	3.300219
133.942968	3652.204973	6.513408	-0.027433	3.303650
134.165960	3660.218784	6.518413	-0.027480	3.307084
134.273749	3668.268851	6.523418	-0.027505	3.310525
134.420285	3676.341488	6.528422	-0.027538	3.313974
134.656380	3684.365559	6.533427	-0.027587	3.317402
134.851333	3692.373803	6.538432	-0.027629	3.320818
134.993227	3700.328227	6.543437	-0.027661	3.324206
135.244459	3708.409902	6.548442	-0.027713	3.327648
135.339739	3716.429855	6.553446	-0.027736	3.331055
135.288864	3724.489303	6.558451	-0.027732	3.334470
135.575030	3732.503916	6.563456	-0.027791	3.337874
135.746545	3740.516923	6.568461	-0.027828	3.341270
135.895025	3748.543135	6.573466	-0.027861	3.344668
136.163226	3756.556086	6.578470	-0.027916	3.348060
136.326509	3764.645647	6.583475	-0.027952	3.351478
136.441577	3772.674322	6.588480	-0.027979	3.354865
136.746598	3780.661384	6.593485	-0.028041	3.358237
136.835636	3788.705681	6.598490	-0.028063	3.361623
136.988609	3796.709514	6.603494	-0.028097	3.364990
137.193688	3804.751221	6.608499	-0.028141	3.368372
137.562344	3812.787127	6.613504	-0.028215	3.371754
137.627200	3820.839301	6.618509	-0.028232	3.375128
137.874681	3828.862373	6.623514	-0.028284	3.378493
137.947596	3836.876255	6.628518	-0.028303	3.381845
138.358940	3844.882921	6.633523	-0.028385	3.385202
138.523173	3852.936601	6.638528	-0.028421	3.388567
138.665982	3860.981438	6.643533	-0.028453	3.391924
138.967300	3869.098273	6.648538	-0.028514	3.395314
138.926708	3877.045508	6.653542	-0.028512	3.398617
139.191076	3885.049356	6.658547	-0.028567	3.401951
139.357760	3893.039246	6.663552	-0.028603	3.405273
139.306560	3901.075528	6.668557	-0.028599	3.408603
139.605704	3909.087497	6.673562	-0.028660	3.411932
139.625829	3917.138895	6.678566	-0.028669	3.415265
139.787609	3925.152446	6.683571	-0.028705	3.418583
139.926493	3933.165926	6.688576	-0.028736	3.421898
139.956732	3941.216640	6.693581	-0.028747	3.425220
140.308017	3949.219248	6.698586	-0.028818	3.428531
140.345803	3957.262300	6.703590	-0.028830	3.431844
140.536325	3965.309006	6.708595	-0.028871	3.435161
140.810908	3973.317205	6.713600	-0.028928	3.438462
140.924595	3981.328839	6.718605	-0.028954	3.441755
141.011886	3989.367103	6.723610	-0.028976	3.445055
141.115182	3997.379815	6.728614	-0.029000	3.448342
141.049072	4005.461987	6.733619	-0.028993	3.451649
141.326833	4013.482916	6.738624	-0.029051	3.454939
141.473210	4021.484745	6.743629	-0.029083	3.458214
141.700708	4029.547400	6.748634	-0.029131	3.461513
141.610035	4037.521568	6.753638	-0.029120	3.464762
141.908549	4045.578652	6.758643	-0.029181	3.468055
142.084483	4053.624151	6.763648	-0.029219	3.471336
142.154447	4061.676556	6.768653	-0.029237	3.474613
142.382601	4069.682550	6.773658	-0.029285	3.477874
142.428085	4077.700614	6.778662	-0.029299	3.481130
142.752526	4085.647981	6.783667	-0.029365	3.484363
142.836283	4093.700462	6.788672	-0.029386	3.487629
143.055004	4101.736823	6.793677	-0.029432	3.490889
143.170206	4109.783505	6.798682	-0.029459	3.494146
143.157941	4117.811380	6.803686	-0.029462	3.497389
143.208981	4125.824753	6.808691	-0.029477	3.500626
143.638307	4133.806098	6.813696	-0.029562	3.503858
143.774421	4141.851088	6.818701	-0.029593	3.507104
143.860567	4149.902033	6.823706	-0.029614	3.510347
143.903871	4157.936594	6.828710	-0.029628	3.513580
143.971319	4165.966617	6.833715	-0.029646	3.516808
144.111011	4173.973612	6.838720	-0.029677	3.520026
144.155826	4181.950879	6.843725	-0.029691	3.523227
144.511785	4190.017681	6.848730	-0.029762	3.526470
144.669182	4198.011236	6.853734	-0.029797	3.529675
144.755579	4206.106559	6.858739	-0.029819	3.532915
144.839850	4214.143080	6.863744	-0.029840	3.536129
144.879798	4222.122240	6.868749	-0.029853	3.539316
145.211009	4230.160267	6.873754	-0.029920	3.542532
145.252841	4238.177356	6.878758	-0.029933	3.545728
145.723347	4246.186026	6.883763	-0.030026	3.548930
145.671851	4254.333079	6.888768	-0.030022	3.552169
145.639147	4262.347034	6.893773	-0.030021	3.555353
145.900723	4270.328958	6.898778	-0.030075	3.558530
146.063861	4278.321511	6.903782	-0.030111	3.561706
146.117479	4286.320718	6.908787	-0.030126	3.564878
146.469025	4294.320068	6.913792	-0.030197	3.568055
146.407488	4302.364245	6.918797	-0.030191	3.571236
146.605992	4310.432031	6.923802	-0.030233	3.574431
146.717077	4318.405184	6.928806	-0.030259	3.577583
146.793655	4326.446525	6.933811	-0.030279	3.580758
147.063164	4334.463556	6.938816	-0.030335	3.583926
147.145084	4342.464172	6.943821	-0.030355	3.587080
147.464625	4350.509416	6.948826	-0.030420	3.590255
147.680044	4358.531329	6.953830	-0.030466	3.593415
147.838512	4366.566900	6.958835	-0.030501	3.596576
147.908127	4374.569054	6.963840	-0.030519	3.599718
148.056728	4382.564611	6.968845	-0.030552	3.602858
148.184211	4390.627721	6.973850	-0.030581	3.606021
148.296812	4398.601690	6.978854	-0.030608	3.609145
148.630262	4406.658760	6.983859	-0.030675	3.612305
148.852631	4414.730923	6.988864	-0.030722	3.615466
148.901861	4422.688900	6.993869	-0.030736	3.618574
148.998413	4430.772119	6.998874	-0.030760	3.621730
149.053853	4438.767559	7.003878	-0.030776	3.624847
149.052963	4446.801138	7.008883	-0.030781	3.627976
149.209194	4454.861975	7.013888	-0.030815	3.631116
149.240606	4462.907239	7.018893	-0.030827	3.634244
149.577343	4470.919721	7.023898	-0.030895	3.637365
149.585772	4478.903262	7.028902	-0.030902	3.640464
149.866517	4486.906194	7.033907	-0.030959	3.643574
150.043349	4494.941811	7.038912	-0.030998	3.646692
150.043112	4502.942505	7.043917	-0.031003	3.649788
150.339772	4511.016861	7.048922	-0.031064	3.652919
150.355261	4519.052849	7.053926	-0.031072	3.656024
150.536371	4527.041509	7.058931	-0.031111	3.659113
150.662006	4535.090173	7.063936	-0.031140	3.662221
150.814833	4543.064475	7.068941	-0.031174	3.665299
151.073818	4551.124350	7.073946	-0.031227	3.668409
151.211697	4559.144155	7.078950	-0.031258	3.671498
151.435368	4567.177201	7.083955	-0.031305	3.674592
151.482657	4575.218379	7.088960	-0.031320	3.677682
151.498864	4583.206573	7.093965	-0.031328	3.680748
151.857428	4591.217722	7.098970	-0.031400	3.683829
151.924425	4599.249414	7.103974	-0.031418	3.686908
151.935993	4607.253183	7.108979	-0.031426	3.689972
151.999529	4615.330410	7.113984	-0.031443	3.693064
152.246872	4623.344307	7.118989	-0.031494	3.696132
152.604904	4631.316815	7.123994	-0.031566	3.699186
152.528957	4639.353964	7.128998	-0.031558	3.702250
152.769102	4647.362361	7.134003	-0.031608	3.705309
152.841354	4655.419579	7.139008	-0.031627	3.708380
152.810953	4663.482791	7.144013	-0.031626	3.711448
153.077338	4671.572890	7.149018	-0.031681	3.714531
153.215923	4679.521895	7.154022	-0.031712	3.717555
153.491667	4687.475200	7.159027	-0.031769	3.720581
153.445114	4695.519999	7.164032	-0.031766	3.723631
153.445206	4703.509068	7.169037	-0.031771	3.726659
153.891809	4711.509172	7.174042	-0.031860	3.729700
153.885634	4719.567065	7.179046	-0.031864	3.732749
154.141112	4727.603411	7.184051	-0.031917	3.735793
154.264549	4735.625009	7.189056	-0.031945	3.738827
154.385422	4743.653344	7.194061	-0.031973	3.741860
154.606595	4751.677819	7.199066	-0.032020	3.744892
154.717515	4759.694252	7.204070	-0.032046	3.747916
154.722397	4767.732952	7.209075	-0.032052	3.750943
154.860459	4775.793948	7.214080	-0.032083	3.753979
155.032536	4783.773859	7.219085	-0.032121	3.756983
155.240939	4791.820355	7.224090	-0.032165	3.760010
155.259200	4799.797772	7.229094	-0.032174	3.763005
155.635722	4807.824520	7.234099	-0.032249	3.766024
155.897814	4815.857384	7.239104	-0.032304	3.769040
155.977339	4823.936305	7.244109	-0.032324	3.772067
156.043955	4831.945739	7.249114	-0.032342	3.775065
156.098100	4839.940610	7.254118	-0.032357	3.778055
156.417882	4847.954223	7.259123	-0.032422	3.781055
156.377239	4855.975975	7.264128	-0.032420	3.784048
156.425790	4863.989500	7.269133	-0.032434	3.787038
156.819438	4872.040699	7.274138	-0.032513	3.790047
156.869200	4880.101374	7.279142	-0.032528	3.793049
157.008723	4888.089254	7.284147	-0.032559	3.796024
157.165929	4896.084941	7.289152	-0.032594	3.799000
157.470440	4904.075749	7.294157	-0.032656	3.801975
157.542308	4912.096750	7.299162	-0.032675	3.804954
157.705800	4920.141437	7.304166	-0.032710	3.807941
157.641004	4928.173844	7.309171	-0.032704	3.810916
157.640878	4936.221389	7.314176	-0.032709	3.813896
157.745706	4944.196546	7.319181	-0.032734	3.816849
158.213997	4952.209263	7.324186	-0.032827	3.819822
158.471473	4960.202552	7.329190	-0.032880	3.822780
158.458653	4968.227851	7.334195	-0.032883	3.825742
158.522581	4976.301544	7.339200	-0.032900	3.828722
158.908474	4984.281818	7.344205	-0.032977	3.831671
158.877592	4992.370164	7.349210	-0.032977	3.834649
158.991759	5000.349623	7.354214	-0.033004	3.837588
159.390547	5008.358235	7.359219	-0.033083	3.840541
159.360208	5016.325116	7.364224	-0.033083	3.843468
159.274375	5024.413471	7.369229	-0.033073	3.846435
159.688207	5032.401759	7.374234	-0.033155	3.849374
159.774626	5040.438452	7.379238	-0.033177	3.852322
159.921473	5048.504421	7.384243	-0.033209	3.855280
160.107269	5056.475513	7.389248	-0.033249	3.858201
160.296880	5064.505468	7.394253	-0.033290	3.861142
160.377287	5072.508327	7.399258	-0.033310	3.864068
160.475053	5080.581344	7.404262	-0.033334	3.867018
160.915341	5088.593088	7.409267	-0.033421	3.869950
160.912185	5096.806546	7.414272	-0.033426	3.872945
160.971887	5104.856654	7.419277	-0.033443	3.875879
161.216095	5112.770814	7.424282	-0.033494	3.878765
161.363348	5120.754578	7.429286	-0.033526	3.881672
161.218820	5128.707632	7.434291	-0.033505	3.884560
161.508011	5136.774933	7.439296	-0.033564	3.887496
161.673719	5144.710476	7.444301	-0.033600	3.890379
161.971207	5152.791387	7.449306	-0.033661	3.893316
161.752275	5160.830849	7.454310	-0.033626	3.896225
161.988694	5168.788441	7.459315	-0.033675	3.899112
162.188374	5176.841997	7.464320	-0.033718	3.902030
162.159981	5184.825496	7.469325	-0.033718	3.904916
162.539682	5192.875762	7.474330	-0.033794	3.907832
162.685080	5200.876895	7.479334	-0.033826	3.910724
162.946236	5208.915260	7.484339	-0.033880	3.913629
163.061882	5216.973273	7.489344	-0.033907	3.916536
163.181817	5224.914004	7.494349	-0.033935	3.919399
163.370929	5232.936881	7.499354	-0.033976	3.922290
163.384607	5240.936496	7.504358	-0.033984	3.925168
163.587634	5248.984525	7.509363	-0.034027	3.928065
163.572024	5257.069631	7.514368	-0.034029	3.930969
163.670360	5265.032292	7.519373	-0.034053	3.933828
163.949645	5273.063132	7.524378	-0.034110	3.936714
164.063399	5281.021982	7.529382	-0.034137	3.939568
163.985549	5289.093862	7.534387	-0.034128	3.942458
164.222123	5297.093226	7.539392	-0.034177	3.945324
164.537614	5305.098115	7.544397	-0.034241	3.948193
164.679838	5313.163805	7.549402	-0.034273	3.951077
164.770616	5321.201242	7.554406	-0.034296	3.953949
164.917872	5329.236563	7.559411	-0.034328	3.956819
165.053468	5337.227551	7.564416	-0.034359	3.959670
165.062744	5345.223463	7.569421	-0.034366	3.962520
165.566052	5353.209234	7.574426	-0.034465	3.965371
165.566090	5361.243557	7.579430	-0.034471	3.968230
165.748135	5369.294309	7.584435	-0.034510	3.971095
165.848675	5377.319677	7.589440	-0.034534	3.973948
166.079771	5385.338516	7.594445	-0.034583	3.976799
166.287503	5393.363436	7.599450	-0.034627	3.979649
166.145798	5401.389489	7.604454	-0.034606	3.982492
166.412716	5409.372119	7.609459	-0.034661	3.985324
166.488552	5417.408275	7.614464	-0.034680	3.988171
166.537170	5425.417926	7.619469	-0.034695	3.991005
166.820792	5433.504600	7.624474	-0.034753	3.993868
167.000889	5441.535660	7.629478	-0.034792	3.996708
167.022955	5449.515171	7.634483	-0.034801	3.999525
167.292706	5457.519121	7.639488	-0.034857	4.002352
167.269549	5465.489005	7.644493	-0.034858	4.005161
167.486947	5473.592800	7.649498	-0.034904	4.008019
167.454651	5481.594833	7.654502	-0.034903	4.010835
167.723647	5489.638688	7.659507	-0.034959	4.013669
167.806944	5497.706419	7.664512	-0.034980	4.016505
168.041210	5505.631801	7.669517	-0.035029	4.019293
167.972426	5513.691886	7.674522	-0.035021	4.022121
168.460474	5521.651150	7.679526	-0.035118	4.024920
168.502884	5529.701668	7.684531	-0.035131	4.027742
168.699610	5537.719905	7.689536	-0.035173	4.030554
168.729881	5545.825136	7.694541	-0.035184	4.033391
168.900693	5553.900540	7.699546	-0.035221	4.036218
169.041945	5561.821222	7.704550	-0.035253	4.038988
169.157765	5569.811093	7.709555	-0.035280	4.041781
169.421443	5577.794859	7.714560	-0.035334	4.044571
169.341915	5585.818555	7.719565	-0.035325	4.047368
169.526437	5593.861685	7.724570	-0.035365	4.050174
169.687900	5601.887239	7.729574	-0.035400	4.052972
170.148843	5609.895979	7.734579	-0.035491	4.055766
170.039493	5617.914503	7.739584	-0.035476	4.058554
170.030622	5625.908268	7.744589	-0.035480	4.061332
170.331564	5633.915372	7.749594	-0.035542	4.064117
170.313029	5641.952956	7.754598	-0.035543	4.066907
170.403798	5649.933053	7.759603	-0.035566	4.069676
170.577938	5658.023352	7.764608	-0.035604	4.072483
170.698220	5666.003384	7.769613	-0.035631	4.075248
171.097053	5674.032679	7.774618	-0.035711	4.078033
171.064248	5682.060612	7.779622	-0.035710	4.080810
171.222766	5690.006844	7.784627	-0.035745	4.083559
171.338467	5698.113004	7.789632	-0.035772	4.086360
171.228604	5706.083534	7.794637	-0.035757	4.089110
171.694663	5714.138988	7.799642	-0.035849	4.091895
171.700509	5722.123061	7.804646	-0.035856	4.094648
171.715840	5730.159288	7.809651	-0.035864	4.097416
171.944511	5738.189955	7.814656	-0.035912	4.100184
171.940626	5746.199735	7.819661	-0.035917	4.102939
172.172779	5754.182209	7.824666	-0.035965	4.105687
172.399929	5762.205778	7.829670	-0.036013	4.108446
172.683577	5770.266350	7.834675	-0.036071	4.111217
172.729049	5778.328763	7.839680	-0.036085	4.113984
172.854135	5786.347175	7.844685	-0.036114	4.116735
173.204927	5794.322443	7.849690	-0.036184	4.119472
173.162029	5802.374399	7.854694	-0.036182	4.122228
173.310567	5810.320583	7.859699	-0.036215	4.124949
173.583279	5818.391713	7.864704	-0.036271	4.127712
173.761326	5826.372226	7.869709	-0.036310	4.130442
173.913243	5834.460570	7.874714	-0.036343	4.133206
174.107019	5842.442142	7.879718	-0.036385	4.135932
174.097021	5850.451080	7.884723	-0.036388	4.138663
174.243373	5858.527508	7.889728	-0.036421	4.141417
174.056807	5866.469973	7.894733	-0.036392	4.144120
174.370121	5874.553944	7.899738	-0.036455	4.146875
174.527569	5882.551607	7.904742	-0.036490	4.149597
174.693922	5890.580008	7.909747	-0.036526	4.152328
174.835075	5898.599941	7.914752	-0.036558	4.155054
174.885646	5906.597994	7.919757	-0.036573	4.157769
175.013423	5914.644667	7.924762	-0.036602	4.160500
175.036983	5922.620121	7.929766	-0.036612	4.163204
175.275744	5930.642281	7.934771	-0.036662	4.165925
175.497926	5938.670354	7.939776	-0.036709	4.168645
175.475997	5946.708326	7.944781	-0.036710	4.171365
175.904421	5954.700390	7.949786	-0.036795	4.174072
175.830822	5962.747868	7.954790	-0.036787	4.176790
175.890915	5970.749882	7.959795	-0.036803	4.179493
176.145149	5978.778464	7.964800	-0.036856	4.182205
176.360244	5986.761793	7.969805	-0.036901	4.184899
176.391763	5994.813806	7.974810	-0.036913	4.187613
176.405163	6002.803033	7.979814	-0.036921	4.190304
176.758422	6010.933988	7.984819	-0.036992	4.193045
176.722702	6018.986313	7.989824	-0.036991	4.195753
176.613213	6026.894740	7.994829	-0.036976	4.198410
177.104998	6034.890445	7.999834	-0.037073	4.201101
177.189055	6042.815934	8.004838	-0.037093	4.203763
177.411102	6050.912526	8.009843	-0.037140	4.206481
177.627257	6058.903790	8.014848	-0.037186	4.209163
177.640773	6066.930736	8.019853	-0.037194	4.211852
177.870684	6075.018678	8.024858	-0.037242	4.214563
177.837847	6082.984611	8.029862	-0.037241	4.217228
177.981719	6090.976374	8.034867	-0.037273	4.219902
178.177195	6099.007229	8.039872	-0.037315	4.222588
178.251172	6107.002034	8.044877	-0.037334	4.225259
178.577929	6115.044018	8.049882	-0.037401	4.227946
178.832998	6123.047498	8.054886	-0.037454	4.230618
178.784159	6131.142819	8.059891	-0.037450	4.233316
178.977246	6139.156563	8.064896	-0.037491	4.235988
178.911381	6147.090075	8.069901	-0.037484	4.238629
179.160361	6155.122719	8.074906	-0.037536	4.241303
179.181563	6163.113507	8.079910	-0.037545	4.243961
179.332018	6171.125392	8.084915	-0.037579	4.246624
179.691529	6179.146837	8.089920	-0.037651	4.249291
179.671256	6187.190679	8.094925	-0.037653	4.251961
179.990863	6195.243324	8.099930	-0.037718	4.254634
179.866684	6203.299272	8.104934	-0.037700	4.257303
179.875912	6211.267957	8.109939	-0.037707	4.259943
180.102456	6219.299841	8.114944	-0.037755	4.262604
180.370240	6227.297027	8.119949	-0.037810	4.265252
180.583611	6235.357432	8.124954	-0.037855	4.267919
180.626989	6243.367003	8.129958	-0.037869	4.270566
180.970927	6251.402953	8.134963	-0.037938	4.273222
181.059463	6259.493329	8.139968	-0.037960	4.275893
180.884960	6267.413834	8.144973	-0.037933	4.278503
181.178305	6275.443582	8.149978	-0.037993	4.281152
181.178141	6283.411996	8.154982	-0.037998	4.283777
181.318573	6291.454780	8.159987	-0.038030	4.286426
181.567105	6299.458107	8.164992	-0.038081	4.289061
181.607376	6307.505875	8.169997	-0.038094	4.291707
181.851680	6315.545961	8.175002	-0.038145	4.294351
181.873279	6323.572821	8.180006	-0.038155	4.296987
181.996300	6331.552660	8.185011	-0.038183	4.299606
182.196406	6339.611733	8.190016	-0.038226	4.302251
182.196669	6347.596814	8.195021	-0.038231	4.304868
182.551175	6355.625976	8.200026	-0.038302	4.307501
182.671557	6363.648572	8.205030	-0.038330	4.310128
182.537961	6371.670629	8.210035	-0.038311	4.312751
182.820976	6379.676361	8.215040	-0.038369	4.315371
182.889422	6387.668140	8.220045	-0.038387	4.317983
183.077181	6395.665887	8.225050	-0.038427	4.320596
183.258548	6403.693583	8.230054	-0.038466	4.323217
183.447543	6411.708826	8.235059	-0.038507	4.325833
183.541079	6419.725386	8.240064	-0.038530	4.328447
183.574968	6427.766372	8.245069	-0.038542	4.331066
183.712833	6435.801334	8.250074	-0.038573	4.333683
183.647508	6443.801480	8.255078	-0.038566	4.336286
183.703005	6451.773078	8.260083	-0.038582	4.338878
184.078015	6459.834908	8.265088	-0.038657	4.341501
184.128181	6467.787485	8.270093	-0.038671	4.344084
184.308986	6475.867164	8.275098	-0.038711	4.346708
184.453420	6483.863027	8.280102	-0.038743	4.349302
184.576813	6491.908475	8.285107	-0.038771	4.351911
184.760377	6500.030840	8.290112	-0.038811	4.354544
184.749410	6507.994308	8.295117	-0.038814	4.357123
184.875968	6515.902810	8.300122	-0.038843	4.359683
185.201975	6523.926980	8.305126	-0.038909	4.362280
185.252553	6531.896733	8.310131	-0.038924	4.364856
185.507099	6539.978444	8.315136	-0.038977	4.367468
185.674749	6547.972939	8.320141	-0.039013	4.370050
185.986620	6556.005309	8.325146	-0.039077	4.372644
186.076334	6564.062257	8.330150	-0.039099	4.375242
185.994055	6572.037115	8.335155	-0.039089	4.377811
186.320829	6580.077942	8.340160	-0.039155	4.380403
186.208030	6588.067648	8.345165	-0.039140	4.382974
186.404040	6596.080708	8.350170	-0.039182	4.385553
186.611325	6604.110026	8.355174	-0.039226	4.388135
186.707633	6612.090721	8.360179	-0.039249	4.390700
186.860845	6620.160719	8.365184	-0.039283	4.393292
186.914662	6628.185693	8.370189	-0.039298	4.395868
187.174485	6636.185598	8.375194	-0.039352	4.398435
187.189872	6644.198308	8.380198	-0.039360	4.401004
187.277227	6652.192093	8.385203	-0.039382	4.403565
187.645064	6660.211311	8.390208	-0.039456	4.406134
187.659797	6668.208909	8.395213	-0.039464	4.408693
187.718513	6676.252452	8.400218	-0.039480	4.411266
187.925733	6684.318880	8.405222	-0.039524	4.413845
187.942733	6692.323687	8.410227	-0.039533	4.416402
188.095490	6700.332999	8.415232	-0.039567	4.418959
188.170864	6708.377570	8.420237	-0.039586	4.421526
188.324348	6716.373764	8.425242	-0.039620	4.424077
188.378471	6724.389843	8.430246	-0.039636	4.426631
188.553661	6732.419586	8.435251	-0.039674	4.429190
188.839941	6740.473037	8.440256	-0.039732	4.431754
188.947203	6748.501447	8.445261	-0.039758	4.434309
189.165166	6756.530025	8.450266	-0.039804	4.436862
189.285262	6764.473283	8.455270	-0.039831	4.439387
189.398478	6772.514635	8.460275	-0.039858	4.441941
189.698070	6780.454824	8.465280	-0.039919	4.444462
189.692230	6788.517938	8.470285	-0.039923	4.447020
189.907967	6796.523673	8.475290	-0.039969	4.449559
190.000894	6804.609594	8.480294	-0.039992	4.452121
189.824139	6812.601097	8.485299	-0.039964	4.454651
190.250659	6820.646720	8.490304	-0.040049	4.457198
190.443170	6828.604248	8.495309	-0.040090	4.459716
190.518901	6836.618167	8.500314	-0.040110	4.462249
190.632434	6844.621397	8.505318	-0.040136	4.464778
190.840356	6852.633047	8.510323	-0.040180	4.467309
190.947759	6860.699979	8.515328	-0.040206	4.469855
190.778958	6868.690550	8.520333	-0.040180	4.472374
190.971943	6876.703302	8.525338	-0.040221	4.474900
191.337637	6884.743543	8.530342	-0.040294	4.477435
191.319024	6892.668672	8.535347	-0.040296	4.479930
191.426286	6900.760633	8.540352	-0.040322	4.482476
191.641422	6908.706174	8.545357	-0.040367	4.484976
191.706910	6916.776010	8.550362	-0.040385	4.487512
191.923814	6924.766409	8.555366	-0.040430	4.490023
192.102147	6932.796569	8.560371	-0.040469	4.492545
192.207491	6940.863873	8.565376	-0.040494	4.495076
192.292180	6948.848338	8.570381	-0.040515	4.497581
192.509287	6956.852007	8.575386	-0.040561	4.500090
192.725457	6964.861242	8.580391	-0.040607	4.502599
192.635943	6972.848831	8.585395	-0.040595	4.505100
192.840402	6980.929095	8.590400	-0.040639	4.507628
192.934511	6988.913064	8.595405	-0.040662	4.510125
193.055003	6996.979220	8.600410	-0.040690	4.512647
193.255417	7005.040297	8.605415	-0.040732	4.515165
193.421531	7012.942182	8.610419	-0.040769	4.517633
193.592770	7020.996548	8.615424	-0.040806	4.520146
193.601835	7028.985593	8.620429	-0.040813	4.522637
193.794651	7036.960672	8.625434	-0.040854	4.525123
193.764837	7045.005974	8.630439	-0.040854	4.527630
193.891024	7052.990447	8.635443	-0.040883	4.530116
194.216288	7061.088420	8.640448	-0.040949	4.532636
194.269862	7069.070306	8.645453	-0.040964	4.535118
194.503111	7077.106693	8.650458	-0.041013	4.537616
194.452567	7085.105126	8.655463	-0.041009	4.540101
194.655947	7093.082269	8.660467	-0.041052	4.542578
195.090488	7101.111832	8.665472	-0.041139	4.545070
194.704956	7109.163655	8.670477	-0.041072	4.547567
194.978191	7117.156761	8.675482	-0.041129	4.550045
195.227920	7125.230068	8.680487	-0.041181	4.552546
195.293700	7133.193857	8.685491	-0.041198	4.555012
195.606567	7141.248606	8.690496	-0.041262	4.557505
195.766807	7149.178341	8.695501	-0.041297	4.559957
195.700207	7157.209399	8.700506	-0.041290	4.562440
195.933536	7165.230403	8.705511	-0.041339	4.564918
196.097099	7173.251089	8.710515	-0.041375	4.567394
196.337092	7181.284003	8.715520	-0.041425	4.569874
196.489956	7189.311574	8.720525	-0.041459	4.572350
196.603915	7197.369026	8.725530	-0.041485	4.574834
196.625185	7205.355189	8.730535	-0.041495	4.577294
196.727773	7213.334260	8.735539	-0.041519	4.579751
196.814414	7221.449624	8.740544	-0.041541	4.582249
196.814616	7229.380848	8.745549	-0.041546	4.584688
196.969013	7237.430709	8.750554	-0.041580	4.587163
197.029811	7245.466905	8.755559	-0.041597	4.589632
197.288435	7253.465353	8.760563	-0.041651	4.592089
197.637637	7261.550437	8.765568	-0.041721	4.594570
197.561784	7269.542010	8.770573	-0.041712	4.597022
197.642895	7277.485644	8.775578	-0.041733	4.599457
197.631419	7285.549829	8.780583	-0.041736	4.601928
197.806806	7293.444799	8.785587	-0.041774	4.604346
198.029765	7301.565337	8.790592	-0.041821	4.606832
198.170347	7309.546489	8.795597	-0.041852	4.609274
198.318811	7317.603422	8.800602	-0.041886	4.611737
198.374070	7325.605494	8.805607	-0.041901	4.614183
198.518345	7333.646589	8.810611	-0.041933	4.616639
198.886967	7341.617367	8.815616	-0.042007	4.619072
198.749271	7349.650713	8.820621	-0.041987	4.621523
199.012710	7357.628037	8.825626	-0.042042	4.623956
199.180881	7365.660842	8.830631	-0.042078	4.626404
199.372145	7373.682617	8.835635	-0.042119	4.628848
199.461279	7381.774253	8.840640	-0.042141	4.631311
199.647558	7389.753368	8.845645	-0.042181	4.633739
199.732633	7397.762275	8.850650	-0.042203	4.636175
199.804681	7405.757949	8.855655	-0.042222	4.638605
199.958480	7413.765195	8.860659	-0.042256	4.641038
200.440531	7421.806162	8.865664	-0.042351	4.643480
200.447075	7429.774370	8.870669	-0.042357	4.645898
200.247562	7437.789488	8.875674	-0.042326	4.648329
200.630706	7445.832897	8.880679	-0.042402	4.650768
200.589393	7453.858895	8.885683	-0.042400	4.653200
200.879276	7461.893161	8.890688	-0.042459	4.655633
200.798453	7469.897564	8.895693	-0.042450	4.658056
200.973610	7477.872908	8.900698	-0.042488	4.660468
201.025247	7485.929478	8.905703	-0.042503	4.662904
201.096652	7493.869470	8.910707	-0.042521	4.665304
201.561496	7501.953667	8.915712	-0.042613	4.667745
201.476607	7509.952090	8.920717	-0.042603	4.670160
201.668264	7518.026200	8.925722	-0.042644	4.672596
201.929569	7526.089390	8.930727	-0.042698	4.675028
201.928373	7534.015788	8.935731	-0.042703	4.677417
202.104975	7542.005165	8.940736	-0.042742	4.679824
202.313307	7550.008227	8.945741	-0.042786	4.682233
202.419468	7557.943364	8.950746	-0.042811	4.684621
202.498422	7566.062047	8.955751	-0.042831	4.687063
202.457318	7574.005666	8.960755	-0.042829	4.689452
202.920233	7582.124648	8.965760	-0.042920	4.691891
202.875532	7590.093148	8.970765	-0.042917	4.694284
203.052313	7598.158642	8.975770	-0.042956	4.696705
203.298566	7606.106005	8.980775	-0.043007	4.699089
203.369470	7614.091743	8.985779	-0.043025	4.701483
203.468069	7622.151587	8.990784	-0.043049	4.703899
203.437457	7630.181349	8.995789	-0.043049	4.706304
203.747011	7638.164490	9.000794	-0.043112	4.708694
203.806540	7646.204216	9.005799	-0.043128	4.711100
203.922716	7654.211973	9.010803	-0.043155	4.713495
204.242835	7662.237989	9.015808	-0.043220	4.715893
204.427148	7670.239958	9.020813	-0.043260	4.718284
204.365991	7678.216859	9.025818	-0.043254	4.720666
204.507203	7686.294682	9.030823	-0.043286	4.723077
204.565905	7694.271310	9.035827	-0.043302	4.725456
204.743388	7702.315872	9.040832	-0.043341	4.727855
205.126059	7710.337104	9.045837	-0.043417	4.730244
205.207628	7718.367117	9.050842	-0.043438	4.732636
205.369489	7726.451282	9.055847	-0.043473	4.735043
205.354713	7734.380527	9.060851	-0.043476	4.737402
205.559015	7742.419813	9.065856	-0.043519	4.739793
205.639265	7750.400029	9.070861	-0.043540	4.742165
205.689016	7758.411296	9.075866	-0.043554	4.744545
205.820294	7766.475828	9.080871	-0.043584	4.746940
205.961063	7774.418344	9.085875	-0.043616	4.749297
206.154899	7782.521221	9.090880	-0.043657	4.751700
206.197289	7790.562385	9.095885	-0.043671	4.754084
206.491949	7798.556685	9.100890	-0.043731	4.756453
206.514044	7806.520375	9.105895	-0.043740	4.758812
206.592796	7814.531929	9.110899	-0.043760	4.761183
206.867754	7822.519215	9.115904	-0.043817	4.763546
207.124829	7830.548374	9.120909	-0.043870	4.765920
207.245313	7838.530343	9.125914	-0.043898	4.768279
207.129059	7846.605349	9.130919	-0.043882	4.770666
207.351572	7854.606124	9.135923	-0.043929	4.773028
207.529243	7862.664339	9.140928	-0.043967	4.775406
207.572047	7870.609541	9.145933	-0.043981	4.777750
207.751660	7878.614464	9.150938	-0.044019	4.780110
207.836323	7886.703739	9.155943	-0.044041	4.782494
208.028377	7894.619398	9.160947	-0.044082	4.784825
208.164381	7902.748217	9.165952	-0.044112	4.787218
208.197307	7910.694048	9.170957	-0.044124	4.789556
208.246762	7918.737435	9.175962	-0.044139	4.791922
208.391500	7926.713958	9.180967	-0.044171	4.794267
208.483516	7934.775511	9.185971	-0.044193	4.796636
208.826353	7942.740575	9.190976	-0.044263	4.798974
208.924086	7950.785802	9.195981	-0.044286	4.801335
208.906937	7958.749236	9.200986	-0.044288	4.803672
209.256458	7966.817958	9.205991	-0.044359	4.806037
209.156578	7974.802906	9.210995	-0.044346	4.808378
209.229091	7982.860487	9.216000	-0.044365	4.810739
209.386110	7990.366789	9.221005	-0.044399	4.812936
209.427060	7995.084295	9.226010	-0.044410	4.814317

209.515150	7997.718271	9.231015	-0.044428	4.815088
209.632800	7999.009935	9.236019	-0.044451	4.815465
209.860477	7999.427540	9.241024	-0.044494	4.815586
209.724045	8000.490149	9.246029	-0.044469	4.815898
209.981650	8000.552980	9.251034	-0.044517	4.815915
210.151178	8000.563184	9.256039	-0.044549	4.815917
210.024592	8000.534493	9.261043	-0.044526	4.815909
210.209216	8000.475587	9.266048	-0.044560	4.815891
210.182032	8000.564790	9.271053	-0.044555	4.815917
210.363072	8000.586916	9.276058	-0.044589	4.815923
210.322533	8000.464646	9.281063	-0.044582	4.815887
210.427569	8000.562373	9.286067	-0.044602	4.815916
210.617163	8000.416055	9.291072	-0.044637	4.815872
210.377971	8000.485851	9.296077	-0.044593	4.815893
210.442495	8000.503973	9.301082	-0.044605	4.815898
210.622703	8000.516483	9.306087	-0.044639	4.815901
210.493599	8000.578444	9.311091	-0.044615	4.815920
210.675761	8000.526967	9.316096	-0.044649	4.815904
210.740355	8000.480004	9.321101	-0.044661	4.815890
210.686907	8000.595461	9.326106	-0.044651	4.815924
210.682243	8000.492971	9.331111	-0.044651	4.815894
210.772055	8000.584054	9.336115	-0.044668	4.815920
210.859758	8000.491582	9.341120	-0.044684	4.815893
210.754429	8000.579532	9.346125	-0.044665	4.815919
210.797246	8000.489541	9.351130	-0.044673	4.815892
210.905511	8000.585188	9.356135	-0.044693	4.815920
210.921005	8000.584384	9.361139	-0.044696	4.815920
210.950839	8000.490984	9.366144	-0.044702	4.815892
210.962273	8000.542397	9.371149	-0.044704	4.815907
211.177477	8000.571475	9.376154	-0.044744	4.815915
211.079976	8000.496302	9.381159	-0.044726	4.815893
211.233517	8000.590543	9.386163	-0.044755	4.815920
211.319267	8000.517245	9.391168	-0.044771	4.815898
211.387558	8000.476743	9.396173	-0.044784	4.815886
211.201925	8000.603950	9.401178	-0.044750	4.815924
211.263794	8000.497192	9.406183	-0.044761	4.815892
211.406737	8000.580593	9.411187	-0.044788	4.815916
211.343183	8000.514501	9.416192	-0.044777	4.815897
211.179678	8000.591914	9.421197	-0.044746	4.815921
211.129088	8000.474815	9.426202	-0.044737	4.815887
211.194251	8000.527091	9.431207	-0.044749	4.815902
211.194574	8000.549518	9.436211	-0.044750	4.815908
211.529382	8000.583718	9.441216	-0.044812	4.815917
211.286013	8000.537144	9.446221	-0.044767	4.815904
211.290429	8000.497751	9.451226	-0.044768	4.815892
211.425917	8000.592770	9.456231	-0.044793	4.815920
211.509170	8000.469283	9.461235	-0.044809	4.815883
211.461238	8000.505873	9.466240	-0.044800	4.815894
211.738510	8000.601035	9.471245	-0.044852	4.815921
211.531140	8000.606255	9.476250	-0.044814	4.815923
211.546540	8000.520090	9.481255	-0.044817	4.815898
211.572258	8000.494910	9.486259	-0.044822	4.815890
211.571963	8000.514126	9.491264	-0.044822	4.815896
211.550591	8000.522333	9.496269	-0.044818	4.815898
211.601488	8000.481552	9.501274	-0.044827	4.815886
211.666666	8000.499685	9.506279	-0.044840	4.815891
211.680484	8000.625828	9.511283	-0.044843	4.815928
211.720422	8000.422687	9.516288	-0.044850	4.815868
211.644831	8000.599677	9.521293	-0.044836	4.815921
211.710208	8000.598607	9.526298	-0.044849	4.815920
211.778910	8000.493025	9.531303	-0.044862	4.815889
211.874613	8000.615148	9.536307	-0.044880	4.815924
211.934544	8000.612925	9.541312	-0.044891	4.815923
212.068410	8000.512657	9.546317	-0.044916	4.815893
211.842583	8000.611477	9.551322	-0.044874	4.815923
212.047906	8000.536898	9.556327	-0.044913	4.815900
211.880763	8000.523557	9.561331	-0.044882	4.815897
211.859806	8000.525369	9.566336	-0.044878	4.815898
211.777743	8000.493123	9.571341	-0.044863	4.815889
211.914139	8000.508132	9.576346	-0.044888	4.815892
212.221047	8000.519479	9.581351	-0.044946	4.815894
211.931648	8000.622613	9.586355	-0.044892	4.815926
212.106926	8000.441917	9.591360	-0.044925	4.815872
212.142361	8000.582279	9.596365	-0.044931	4.815913
212.026245	8000.540949	9.601370	-0.044910	4.815902
212.069332	8000.538455	9.606375	-0.044918	4.815901
212.008170	8000.507611	9.611379	-0.044907	4.815892
212.035075	8000.547537	9.616384	-0.044912	4.815903
212.108823	8000.475112	9.621389	-0.044926	4.815882
212.025133	8000.630633	9.626394	-0.044911	4.815928
212.224310	8000.410842	9.631399	-0.044948	4.815862
212.051387	8000.596940	9.636403	-0.044916	4.815918
212.252803	8000.530834	9.641408	-0.044954	4.815897
212.293750	8000.600863	9.646413	-0.044961	4.815918
212.074666	8000.614430	9.651418	-0.044921	4.815923
212.359358	8000.513383	9.656423	-0.044974	4.815892
212.372131	8000.481593	9.661427	-0.044976	4.815882
212.385758	8000.542646	9.666432	-0.044979	4.815900
212.351789	8000.549584	9.671437	-0.044973	4.815902
212.313254	8000.603398	9.676442	-0.044966	4.815918
212.251044	8000.527722	9.681447	-0.044955	4.815897
212.223534	8000.612656	9.686451	-0.044950	4.815921
212.567908	8000.638477	9.691456	-0.045014	4.815927
212.460631	8000.526865	9.696461	-0.044994	4.815895
212.612480	8000.610413	9.701466	-0.045023	4.815919
212.578817	8000.507452	9.706471	-0.045016	4.815889
212.625112	8000.613846	9.711475	-0.045025	4.815920
212.821034	8000.545518	9.716480	-0.045062	4.815899
212.439032	8000.519121	9.721485	-0.044991	4.815893
212.460417	8000.534418	9.726490	-0.044995	4.815897
212.615728	8000.631893	9.731495	-0.045024	4.815925
212.432915	8000.582021	9.736499	-0.044990	4.815912
212.649732	8000.532168	9.741504	-0.045031	4.815896
212.662337	8000.623083	9.746509	-0.045033	4.815922
212.618345	8000.514621	9.751514	-0.045025	4.815891
212.581355	8000.516175	9.756519	-0.045019	4.815892
212.466947	8000.533558	9.761523	-0.044997	4.815897
212.644078	8000.422247	9.766528	-0.045031	4.815864
212.444700	8000.606854	9.771533	-0.044994	4.815919
212.583875	8000.426644	9.776538	-0.045020	4.815865
212.742633	8000.519906	9.781543	-0.045049	4.815892
212.720999	8000.595332	9.786547	-0.045046	4.815914
212.823879	8000.635414	9.791552	-0.045065	4.815925
212.882892	8000.476322	9.796557	-0.045076	4.815878
212.659887	8000.637075	9.801562	-0.045035	4.815926
212.507237	8000.435104	9.806567	-0.045006	4.815868
212.772995	8000.616515	9.811571	-0.045056	4.815920
212.841421	8000.619763	9.816576	-0.045069	4.815921
212.572971	8000.605860	9.821581	-0.045019	4.815918
212.813787	8000.495572	9.826586	-0.045064	4.815884
213.041914	8000.522727	9.831591	-0.045107	4.815891
212.799564	8000.626618	9.836595	-0.045062	4.815923
212.882021	8000.536193	9.841600	-0.045077	4.815896
212.947450	8000.594879	9.846605	-0.045090	4.815913
213.027871	8000.606856	9.851610	-0.045105	4.815916
212.991738	8000.535866	9.856615	-0.045098	4.815895
212.936785	8000.594751	9.861619	-0.045088	4.815913
213.043242	8000.518583	9.866624	-0.045108	4.815890
213.013924	8000.498920	9.871629	-0.045103	4.815884
212.995408	8000.619212	9.876634	-0.045100	4.815920
212.961228	8000.529046	9.881639	-0.045094	4.815893
212.916226	8000.529405	9.886643	-0.045085	4.815894
213.059899	8000.628829	9.891648	-0.045112	4.815922
213.004241	8000.537250	9.896653	-0.045102	4.815896
213.007909	8000.531989	9.901658	-0.045103	4.815894
212.948693	8000.446756	9.906663	-0.045092	4.815869
212.884041	8000.619658	9.911667	-0.045080	4.815920
212.990527	8000.534954	9.916672	-0.045100	4.815895
212.938392	8000.492517	9.921677	-0.045091	4.815883
212.860648	8000.625729	9.926682	-0.045076	4.815922
213.031339	8000.423616	9.931687	-0.045108	4.815862
212.921542	8000.612865	9.936691	-0.045088	4.815918
213.097966	8000.538888	9.941696	-0.045121	4.815896
213.053762	8000.603282	9.946701	-0.045113	4.815915
212.982989	8000.503992	9.951706	-0.045100	4.815886
213.071408	8000.528902	9.956711	-0.045117	4.815893
213.186638	8000.640674	9.961715	-0.045138	4.815925
213.218620	8000.524895	9.966720	-0.045144	4.815891
213.264087	8000.538444	9.971725	-0.045153	4.815895
213.324243	8000.509549	9.976730	-0.045164	4.815886
213.289574	8000.551688	9.981735	-0.045158	4.815898
213.215033	8000.593186	9.986739	-0.045144	4.815911
213.113255	8000.505135	9.991744	-0.045126	4.815886
213.218679	8000.491905	9.996749	-0.045145	4.815881
213.251512	8000.552202	10.001754	-0.045152	4.815899
213.057565	8000.532027	10.006759	-0.045116	4.815894
213.109208	8000.600095	10.011763	-0.045126	4.815913
213.257512	8000.551275	10.016768	-0.045153	4.815898
213.294012	8000.514530	10.021773	-0.045160	4.815887
213.096825	8000.551923	10.026778	-0.045124	4.815899
213.245698	8000.520185	10.031783	-0.045152	4.815889
213.408853	8000.502548	10.036787	-0.045182	4.815883
213.403734	8000.552631	10.041792	-0.045181	4.815898
213.442314	8000.423086	10.046797	-0.045189	4.815860
213.409917	8000.519681	10.051802	-0.045183	4.815888
213.511250	8000.425290	10.056807	-0.045202	4.815860
213.325093	8000.582370	10.061811	-0.045167	4.815907
213.496019	8000.432544	10.066816	-0.045199	4.815862
213.428365	8000.520036	10.071821	-0.045187	4.815888
213.375983	8000.503203	10.076826	-0.045177	4.815884
213.464897	8000.641229	10.081831	-0.045194	4.815924
213.423322	8000.515731	10.086835	-0.045187	4.815887
213.294850	8000.636391	10.091840	-0.045163	4.815923
213.317581	8000.551407	10.096845	-0.045167	4.815898
213.468273	8000.523966	10.101850	-0.045195	4.815889
213.513912	8000.495904	10.106855	-0.045204	4.815881
213.310820	8000.506526	10.111859	-0.045166	4.815885
213.438441	8000.640906	10.116864	-0.045190	4.815924
213.654972	8000.500349	10.121869	-0.045231	4.815882
213.443920	8000.509776	10.126874	-0.045192	4.815885
213.529880	8000.526111	10.131879	-0.045208	4.815890
213.620735	8000.536123	10.136883	-0.045225	4.815892
213.480571	8000.531750	10.141888	-0.045199	4.815892
213.405128	8000.524150	10.146893	-0.045185	4.815890
213.417100	8000.526491	10.151898	-0.045188	4.815890
213.496630	8000.508577	10.156903	-0.045203	4.815885
213.445555	8000.530179	10.161907	-0.045193	4.815891
213.725791	8000.549637	10.166912	-0.045246	4.815896
213.600611	8000.538036	10.171917	-0.045222	4.815893
213.329946	8000.603058	10.176922	-0.045172	4.815913
213.571102	8000.425551	10.181927	-0.045217	4.815860
213.506705	8000.623001	10.186931	-0.045206	4.815918
213.453487	8000.425824	10.191936	-0.045196	4.815861
213.520234	8000.542152	10.196941	-0.045208	4.815894
213.499509	8000.530096	10.201946	-0.045205	4.815891
213.732441	8000.539190	10.206951	-0.045248	4.815892
213.533566	8000.632042	10.211955	-0.045211	4.815921
213.589398	8000.423813	10.216960	-0.045222	4.815859
213.569041	8000.501395	10.221965	-0.045218	4.815882
213.492831	8000.548201	10.226970	-0.045204	4.815896
213.592161	8000.382286	10.231975	-0.045223	4.815847
213.590025	8000.426015	10.236979	-0.045223	4.815860
213.672004	8000.524449	10.241984	-0.045238	4.815888
213.604177	8000.541513	10.246989	-0.045226	4.815894
213.603463	8000.553254	10.251994	-0.045226	4.815897
213.642020	8000.385295	10.256999	-0.045233	4.815848
213.455897	8000.607465	10.262003	-0.045199	4.815914
213.606797	8000.326071	10.267008	-0.045227	4.815831
213.832769	8000.489774	10.272013	-0.045269	4.815877
213.701305	8000.372434	10.277018	-0.045245	4.815844
213.618359	8000.367915	10.282023	-0.045229	4.815843
213.611358	8000.431840	10.287027	-0.045228	4.815862
213.608949	8000.553459	10.292032	-0.045228	4.815897
213.675647	8000.594027	10.297037	-0.045241	4.815909
213.704078	8000.624376	10.302042	-0.045246	4.815917
213.727768	8000.550078	10.307047	-0.045251	4.815896
213.413140	8000.548236	10.312051	-0.045192	4.815897
213.492798	8000.531391	10.317056	-0.045207	4.815891
213.734636	8000.518220	10.322061	-0.045252	4.815886
213.795346	8000.540552	10.327066	-0.045264	4.815892
213.698203	8000.295718	10.332071	-0.045246	4.815821
213.724963	8000.496768	10.337075	-0.045251	4.815880
213.662439	8000.488308	10.342080	-0.045240	4.815878
213.669042	8000.625012	10.347085	-0.045241	4.815918
213.730575	8000.554523	10.352090	-0.045253	4.815897
213.794963	8000.454202	10.357095	-0.045265	4.815867
213.670768	8000.565328	10.362099	-0.045242	4.815900
213.809447	8000.444861	10.367104	-0.045268	4.815864
213.905553	8000.541388	10.372109	-0.045286	4.815892
213.682651	8000.418310	10.377114	-0.045245	4.815857
213.732713	8000.391386	10.382119	-0.045254	4.815849
213.808596	8000.517465	10.387123	-0.045268	4.815886
213.978344	8000.539416	10.392128	-0.045300	4.815891
213.813574	8000.529312	10.397133	-0.045270	4.815889
213.774657	8000.550042	10.402138	-0.045263	4.815895
213.858218	8000.473505	10.407143	-0.045278	4.815872
213.850263	8000.607841	10.412147	-0.045277	4.815912
213.831064	8000.444287	10.417152	-0.045274	4.815864
213.744525	8000.515470	10.422157	-0.045258	4.815885
213.753549	8000.551910	10.427162	-0.045260	4.815896
213.778057	8000.438144	10.432167	-0.045264	4.815862
213.873640	8000.594418	10.437171	-0.045282	4.815908
213.786128	8000.547142	10.442176	-0.045266	4.815894
213.815113	8000.531617	10.447181	-0.045272	4.815890
213.786031	8000.534365	10.452186	-0.045266	4.815891
213.900572	8000.551160	10.457191	-0.045288	4.815895
213.918753	8000.613357	10.462195	-0.045292	4.815913
213.859619	8000.527056	10.467200	-0.045281	4.815888
213.823793	8000.405917	10.472205	-0.045274	4.815853
213.699681	8000.493569	10.477210	-0.045251	4.815879
213.771905	8000.414716	10.482215	-0.045265	4.815856
213.709712	8000.536442	10.487219	-0.045253	4.815892
213.856766	8000.537753	10.492224	-0.045281	4.815891
213.814821	8000.465601	10.497229	-0.045273	4.815870
213.697744	8000.377303	10.502234	-0.045252	4.815845
213.976495	8000.536521	10.507239	-0.045304	4.815890
213.900526	8000.327239	10.512243	-0.045290	4.815829
213.733747	8000.374724	10.517248	-0.045259	4.815844
213.831746	8000.394454	10.522253	-0.045277	4.815849
213.843558	8000.390390	10.527258	-0.045280	4.815848
213.805158	8000.532772	10.532263	-0.045273	4.815890
213.849027	8000.523889	10.537267	-0.045281	4.815887
213.956326	8000.543768	10.542272	-0.045301	4.815892
214.007737	8000.633176	10.547277	-0.045311	4.815918
213.908739	8000.529161	10.552282	-0.045293	4.815888
214.035057	8000.534407	10.557287	-0.045316	4.815889
213.790723	8000.516622	10.562291	-0.045271	4.815885
213.807489	8000.548918	10.567296	-0.045274	4.815895
213.771457	8000.501403	10.572301	-0.045268	4.815881
213.942531	8000.534045	10.577306	-0.045300	4.815890
214.145501	8000.533055	10.582311	-0.045338	4.815888
213.971004	8000.532398	10.587315	-0.045305	4.815889
214.069246	8000.512651	10.592320	-0.045324	4.815883
214.057447	8000.480464	10.597325	-0.045322	4.815873
213.847371	8000.517650	10.602330	-0.045283	4.815885
213.950935	8000.429696	10.607335	-0.045302	4.815859
214.095505	8000.519534	10.612339	-0.045329	4.815885
214.132839	8000.431583	10.617344	-0.045337	4.815859
214.195358	8000.640681	10.622349	-0.045348	4.815920
214.119106	8000.549835	10.627354	-0.045334	4.815893
214.109080	8000.430178	10.632359	-0.045333	4.815858
214.058925	8000.547830	10.637363	-0.045324	4.815893
214.069849	8000.453051	10.642368	-0.045326	4.815865
214.056979	8000.389903	10.647373	-0.045323	4.815847
214.036658	8000.344774	10.652378	-0.045320	4.815834
214.103602	8000.299982	10.657383	-0.045332	4.815820
214.025447	8000.445994	10.662387	-0.045318	4.815863
213.960611	8000.551672	10.667392	-0.045306	4.815895
213.926009	8000.507381	10.672397	-0.045300	4.815882
213.922761	8000.502008	10.677402	-0.045300	4.815880
214.162580	8000.639262	10.682407	-0.045344	4.815919
213.993696	8000.606683	10.687411	-0.045313	4.815911
213.918234	8000.529723	10.692416	-0.045299	4.815888
214.142147	8000.503459	10.697421	-0.045341	4.815880
213.967913	8000.637257	10.702426	-0.045309	4.815920
214.007908	8000.530141	10.707431	-0.045316	4.815888
214.184887	8000.604495	10.712435	-0.045350	4.815909
214.236899	8000.537053	10.717440	-0.045359	4.815889
213.999717	8000.579138	10.722445	-0.045315	4.815902
214.175884	8000.578784	10.727450	-0.045348	4.815902
214.179229	8000.418793	10.732455	-0.045349	4.815855
213.982369	8000.617317	10.737459	-0.045313	4.815914
214.020732	8000.549657	10.742464	-0.045320	4.815894
214.086824	8000.524057	10.747469	-0.045332	4.815886
214.077225	8000.596478	10.752474	-0.045331	4.815907
214.227659	8000.530619	10.757479	-0.045359	4.815887
214.333143	8000.612361	10.762483	-0.045379	4.815911
214.309218	8000.496747	10.767488	-0.045375	4.815877
214.109640	8000.640808	10.772493	-0.045338	4.815920
214.343061	8000.510125	10.777498	-0.045381	4.815881
214.421147	8000.530602	10.782503	-0.045396	4.815886
214.105289	8000.625843	10.787507	-0.045337	4.815916
214.202928	8000.546330	10.792512	-0.045356	4.815892
214.079609	8000.542228	10.797517	-0.045333	4.815891
214.183873	8000.523644	10.802522	-0.045352	4.815885
214.152415	8000.539159	10.807527	-0.045347	4.815890
214.230818	8000.498819	10.812531	-0.045361	4.815878
214.333649	8000.537834	10.817536	-0.045381	4.815889
214.291794	8000.492359	10.822541	-0.045373	4.815876
214.448161	8000.587723	10.827546	-0.045402	4.815903
214.270687	8000.426958	10.832551	-0.045369	4.815857
214.113422	8000.630388	10.837555	-0.045341	4.815917
214.200736	8000.529368	10.842560	-0.045357	4.815887
214.305995	8000.540679	10.847565	-0.045377	4.815890
214.497880	8000.533108	10.852570	-0.045413	4.815887
214.344977	8000.545603	10.857575	-0.045384	4.815891
214.309620	8000.612275	10.862579	-0.045378	4.815911
214.222433	8000.546863	10.867584	-0.045362	4.815892
214.454264	8000.428959	10.872589	-0.045405	4.815856
214.315841	8000.623089	10.877594	-0.045380	4.815914
214.535250	8000.401480	10.882599	-0.045420	4.815848
214.296744	8000.552384	10.887603	-0.045376	4.815893
214.322500	8000.538941	10.892608	-0.045381	4.815889
214.415213	8000.354777	10.897613	-0.045399	4.815835
214.326902	8000.520901	10.902618	-0.045382	4.815884
214.450476	8000.538909	10.907623	-0.045406	4.815888
214.293075	8000.549197	10.912627	-0.045376	4.815892
214.374667	8000.540920	10.917632	-0.045392	4.815889
214.360559	8000.502293	10.922637	-0.045389	4.815878
214.181141	8000.530368	10.927642	-0.045356	4.815887
214.302181	8000.411750	10.932647	-0.045379	4.815852
214.315535	8000.423717	10.937651	-0.045381	4.815855
214.559361	8000.448994	10.942656	-0.045427	4.815862
214.633772	8000.516364	10.947661	-0.045441	4.815881
214.492904	8000.533320	10.952666	-0.045415	4.815887
214.643069	8000.529347	10.957671	-0.045443	4.815885
214.606820	8000.431675	10.962675	-0.045436	4.815856
214.624152	8000.556817	10.967680	-0.045440	4.815893
214.609619	8000.325043	10.972685	-0.045437	4.815825
214.391382	8000.515755	10.977690	-0.045397	4.815882
214.474682	8000.551255	10.982695	-0.045413	4.815892
214.372334	8000.520813	10.987699	-0.045394	4.815883
214.537372	8000.549092	10.992704	-0.045425	4.815891
214.751262	8000.511997	10.997709	-0.045465	4.815879
214.381677	8000.545550	11.002714	-0.045396	4.815891
214.438668	8000.627579	11.007719	-0.045407	4.815914
214.331353	8000.496752	11.012723	-0.045387	4.815877
214.591264	8000.522287	11.017728	-0.045436	4.815883
214.583653	8000.543521	11.022733	-0.045434	4.815889
214.467156	8000.603553	11.027738	-0.045413	4.815907
214.632851	8000.541140	11.032743	-0.045444	4.815888
214.522323	8000.520170	11.037747	-0.045423	4.815882
214.505546	8000.450555	11.042752	-0.045420	4.815862
214.500204	8000.631887	11.047757	-0.045420	4.815915
214.382250	8000.487016	11.052762	-0.045398	4.815873
214.432751	8000.551867	11.057767	-0.045407	4.815892
214.360998	8000.590210	11.062771	-0.045394	4.815904
214.597474	8000.582290	11.067776	-0.045438	4.815900
214.410290	8000.531276	11.072781	-0.045404	4.815886
214.490546	8000.522977	11.077786	-0.045419	4.815883
214.503066	8000.563742	11.082791	-0.045421	4.815895
214.579627	8000.428402	11.087795	-0.045436	4.815855
214.537485	8000.517373	11.092800	-0.045428	4.815882
214.681755	8000.520775	11.097805	-0.045455	4.815882
214.628292	8000.520997	11.102810	-0.045445	4.815882
214.568732	8000.518987	11.107815	-0.045434	4.815882
214.600424	8000.635823	11.112819	-0.045440	4.815916
214.582639	8000.502166	11.117824	-0.045437	4.815877
214.505890	8000.500947	11.122829	-0.045423	4.815877
214.301717	8000.528623	11.127834	-0.045385	4.815886
214.360678	8000.503976	11.132839	-0.045396	4.815878
214.289196	8000.614884	11.137843	-0.045383	4.815911
214.343071	8000.486649	11.142848	-0.045393	4.815873
214.733660	8000.534561	11.147853	-0.045466	4.815886
214.746160	8000.610540	11.152858	-0.045469	4.815908
214.561214	8000.541421	11.157863	-0.045435	4.815888
214.648536	8000.520431	11.162867	-0.045451	4.815882
214.785161	8000.552521	11.167872	-0.045477	4.815891
214.898663	8000.356951	11.172877	-0.045498	4.815833
214.391464	8000.478993	11.177882	-0.045404	4.815871
214.739059	8000.542220	11.182887	-0.045469	4.815888
214.631260	8000.624800	11.187891	-0.045449	4.815912
214.527057	8000.615669	11.192896	-0.045430	4.815910
214.725048	8000.442800	11.197901	-0.045466	4.815859
214.764813	8000.655804	11.202906	-0.045474	4.815921
214.646089	8000.514121	11.207911	-0.045452	4.815880
214.512758	8000.473576	11.212915	-0.045427	4.815869
214.781445	8000.454436	11.217920	-0.045478	4.815862
214.660169	8000.510123	11.222925	-0.045455	4.815879
214.652729	8000.415048	11.227930	-0.045454	4.815851
214.795782	8000.369344	11.232935	-0.045481	4.815837
214.594895	8000.543263	11.237939	-0.045444	4.815889
214.651462	8000.514309	11.242944	-0.045454	4.815880
214.666668	8000.506032	11.247949	-0.045457	4.815877
214.694314	8000.521430	11.252954	-0.045463	4.815882
214.643773	8000.539840	11.257959	-0.045453	4.815887
214.674499	8000.536080	11.262963	-0.045459	4.815886
214.535247	8000.398337	11.267968	-0.045433	4.815847
214.700991	8000.419157	11.272973	-0.045464	4.815852
214.655519	8000.539020	11.277978	-0.045456	4.815887
214.763864	8000.409526	11.282983	-0.045477	4.815849
214.771608	8000.415001	11.287987	-0.045478	4.815850
214.737389	8000.523307	11.292992	-0.045472	4.815882
214.626873	8000.581301	11.297997	-0.045452	4.815900
214.634032	8000.573961	11.303002	-0.045453	4.815897
214.748011	8000.526723	11.308007	-0.045475	4.815883
214.746241	8000.525642	11.313011	-0.045474	4.815883
214.808612	8000.492513	11.318016	-0.045486	4.815873
214.812516	8000.509664	11.323021	-0.045487	4.815878
214.709156	8000.618993	11.328026	-0.045468	4.815910
214.786733	8000.627725	11.333031	-0.045483	4.815912
214.699950	8000.521770	11.338035	-0.045467	4.815882
214.595852	8000.624684	11.343040	-0.045447	4.815912
214.744354	8000.511842	11.348045	-0.045475	4.815879
214.737735	8000.631264	11.353050	-0.045474	4.815914
214.825808	8000.418211	11.358055	-0.045491	4.815851
214.613454	8000.597282	11.363059	-0.045451	4.815904
214.721928	8000.565961	11.368064	-0.045472	4.815895
214.832880	8000.545352	11.373069	-0.045493	4.815888
214.865686	8000.530955	11.378074	-0.045499	4.815884
214.790540	8000.640738	11.383079	-0.045485	4.815916
214.849078	8000.527516	11.388083	-0.045496	4.815883
214.807276	8000.526858	11.393088	-0.045488	4.815883
214.893610	8000.533596	11.398093	-0.045505	4.815884
214.685859	8000.632710	11.403098	-0.045466	4.815914
214.650096	8000.545715	11.408103	-0.045460	4.815889
214.757320	8000.549589	11.413107	-0.045480	4.815890
214.824385	8000.522938	11.418112	-0.045492	4.815882
214.905636	8000.514655	11.423117	-0.045508	4.815879
214.757019	8000.627525	11.428122	-0.045480	4.815912
214.785603	8000.494614	11.433127	-0.045486	4.815873
215.017472	8000.500492	11.438131	-0.045529	4.815874
214.755243	8000.625406	11.443136	-0.045480	4.815912
214.726976	8000.537465	11.448141	-0.045475	4.815886
214.675979	8000.536659	11.453146	-0.045466	4.815886
214.781350	8000.433795	11.458151	-0.045486	4.815856
214.709010	8000.542555	11.463155	-0.045473	4.815888
214.795913	8000.484211	11.468160	-0.045489	4.815870
214.880966	8000.347940	11.473165	-0.045505	4.815830
214.767547	8000.584090	11.478170	-0.045484	4.815900
214.920956	8000.596176	11.483175	-0.045513	4.815902
214.886773	8000.499603	11.488179	-0.045506	4.815874
214.794261	8000.533343	11.493184	-0.045489	4.815885
214.960586	8000.620334	11.498189	-0.045521	4.815909
214.944875	8000.537929	11.503194	-0.045518	4.815885
214.895685	8000.514744	11.508199	-0.045509	4.815879
214.550317	8000.463320	11.513203	-0.045445	4.815865
214.579738	8000.600394	11.518208	-0.045450	4.815905
214.777498	8000.538497	11.523213	-0.045487	4.815886
214.597912	8000.651935	11.528218	-0.045454	4.815920
214.783816	8000.549299	11.533223	-0.045489	4.815889
214.677240	8000.507050	11.538227	-0.045469	4.815877
214.781400	8000.622918	11.543232	-0.045489	4.815911
214.733239	8000.522919	11.548237	-0.045480	4.815882
214.585695	8000.583518	11.553242	-0.045453	4.815900
214.878595	8000.532756	11.558247	-0.045507	4.815884
214.790234	8000.638058	11.563251	-0.045491	4.815915
214.747289	8000.507197	11.568256	-0.045483	4.815877
214.678504	8000.528514	11.573261	-0.045471	4.815884
214.674003	8000.522054	11.578266	-0.045470	4.815882
214.723452	8000.520730	11.583271	-0.045479	4.815881
214.762369	8000.526706	11.588275	-0.045487	4.815883
214.846200	8000.582490	11.593280	-0.045502	4.815899
214.765170	8000.554524	11.598285	-0.045488	4.815891
214.777951	8000.550476	11.603290	-0.045490	4.815890
214.826299	8000.541665	11.608295	-0.045499	4.815887
214.867163	8000.530598	11.613299	-0.045507	4.815883
214.939658	8000.546718	11.618304	-0.045521	4.815888
215.051544	8000.423683	11.623309	-0.045542	4.815851
215.000514	8000.529586	11.628314	-0.045532	4.815882
214.866644	8000.455953	11.633319	-0.045508	4.815862
214.809558	8000.525477	11.638323	-0.045497	4.815882
214.808309	8000.510532	11.643328	-0.045497	4.815878
214.903580	8000.538756	11.648333	-0.045515	4.815886
214.816790	8000.614205	11.653338	-0.045499	4.815908
214.944563	8000.428468	11.658343	-0.045523	4.815853
214.944437	8000.549061	11.663347	-0.045523	4.815888
214.891894	8000.548231	11.668352	-0.045514	4.815888
214.931074	8000.546741	11.673357	-0.045521	4.815888
214.911599	8000.619005	11.678362	-0.045518	4.815909
214.920195	8000.545528	11.683367	-0.045519	4.815887
214.847382	8000.400315	11.688371	-0.045506	4.815845
214.953316	8000.495937	11.693376	-0.045526	4.815873
214.935818	8000.609849	11.698381	-0.045523	4.815906
214.776212	8000.561411	11.703386	-0.045493	4.815893
214.905164	8000.547494	11.708391	-0.045517	4.815888
214.749121	8000.521523	11.713395	-0.045488	4.815881
214.946411	8000.594072	11.718400	-0.045525	4.815902
215.086508	8000.524845	11.723405	-0.045552	4.815881
214.990931	8000.506248	11.728410	-0.045534	4.815876
215.009014	8000.424388	11.733415	-0.045537	4.815852
214.970277	8000.438719	11.738419	-0.045530	4.815856
214.822876	8000.533468	11.743424	-0.045503	4.815884
214.859986	8000.517006	11.748429	-0.045510	4.815879
214.650011	8000.517911	11.753434	-0.045471	4.815881
215.015080	8000.551542	11.758439	-0.045539	4.815889
215.078259	8000.512024	11.763443	-0.045551	4.815877
214.928825	8000.513903	11.768448	-0.045524	4.815878
214.911790	8000.435746	11.773453	-0.045521	4.815855
214.940926	8000.624038	11.778458	-0.045526	4.815910
214.799249	8000.520399	11.783463	-0.045500	4.815881
214.767353	8000.533773	11.788467	-0.045494	4.815885
214.830021	8000.595620	11.793472	-0.045506	4.815902
214.971012	8000.532810	11.798477	-0.045533	4.815883
214.624500	8000.531519	11.803482	-0.045468	4.815885
214.812044	8000.626320	11.808487	-0.045503	4.815912
214.873345	8000.614516	11.813491	-0.045515	4.815908
214.695768	8000.543380	11.818496	-0.045482	4.815888
214.729850	8000.561017	11.823501	-0.045489	4.815893
214.900138	8000.578710	11.828506	-0.045520	4.815897
214.890026	8000.498530	11.833511	-0.045519	4.815874
214.774963	8000.627946	11.838515	-0.045498	4.815912
214.820919	8000.449429	11.843520	-0.045506	4.815860
214.891577	8000.601039	11.848525	-0.045520	4.815904
214.877150	8000.556004	11.853530	-0.045517	4.815891
214.915863	8000.605728	11.858535	-0.045524	4.815905
214.933605	8000.516392	11.863539	-0.045528	4.815879
214.877990	8000.607282	11.868544	-0.045518	4.815906
215.015977	8000.564698	11.873549	-0.045544	4.815892
215.042260	8000.535257	11.878554	-0.045549	4.815884
215.102925	8000.540516	11.883559	-0.045560	4.815885
215.086458	8000.397275	11.888563	-0.045557	4.815843
215.066336	8000.534621	11.893568	-0.045554	4.815883
215.094195	8000.563895	11.898573	-0.045559	4.815892
214.754235	8000.531764	11.903578	-0.045496	4.815884
215.075614	8000.450514	11.908583	-0.045556	4.815859
215.143483	8000.403601	11.913587	-0.045569	4.815845
214.816391	8000.534942	11.918592	-0.045508	4.815885
214.930377	8000.537857	11.923597	-0.045529	4.815885
214.856447	8000.629520	11.928602	-0.045516	4.815912
214.900226	8000.541670	11.933607	-0.045524	4.815886
214.659040	8000.627440	11.938611	-0.045479	4.815912
214.803290	8000.509194	11.943616	-0.045506	4.815877
215.053311	8000.650886	11.948621	-0.045553	4.815917
214.833137	8000.526777	11.953626	-0.045512	4.815882
214.891295	8000.529861	11.958631	-0.045523	4.815883
215.069935	8000.518877	11.963635	-0.045557	4.815879
214.822327	8000.538385	11.968640	-0.045511	4.815886
215.052444	8000.543168	11.973645	-0.045554	4.815886
215.128038	8000.609492	11.978650	-0.045568	4.815905
215.240635	8000.410704	11.983655	-0.045589	4.815846
214.983967	8000.533574	11.988659	-0.045541	4.815883
214.883349	8000.518098	11.993664	-0.045523	4.815879
215.233927	8000.552564	11.998669	-0.045588	4.815888
215.150135	8000.587512	12.003674	-0.045573	4.815898
215.117479	8000.518707	12.008679	-0.045567	4.815878
215.259140	8000.399351	12.013683	-0.045593	4.815843
215.070532	8000.560664	12.018688	-0.045559	4.815891
215.210953	8000.323909	12.023693	-0.045585	4.815821
215.027307	8000.474631	12.028698	-0.045551	4.815866
215.201790	8000.483855	12.033703	-0.045584	4.815868
215.238264	8000.506865	12.038707	-0.045590	4.815874
215.192985	8000.563775	12.043712	-0.045582	4.815891
215.071619	8000.533025	12.048717	-0.045560	4.815883
215.025828	8000.631543	12.053722	-0.045552	4.815912
215.004085	8000.536236	12.058727	-0.045548	4.815884
215.256469	8000.504030	12.063731	-0.045595	4.815873
215.226430	8000.548379	12.068736	-0.045589	4.815887
215.036349	8000.456767	12.073741	-0.045554	4.815861
214.907177	8000.597695	12.078746	-0.045530	4.815902
215.102969	8000.521894	12.083751	-0.045567	4.815879
215.063337	8000.499929	12.088755	-0.045560	4.815873
215.100201	8000.606179	12.093760	-0.045567	4.815904
215.203985	8000.500087	12.098765	-0.045586	4.815872
215.100467	8000.572066	12.103770	-0.045567	4.815894
215.134120	8000.615306	12.108775	-0.045574	4.815907
215.160489	8000.523974	12.113779	-0.045579	4.815880
215.181956	8000.583024	12.118784	-0.045583	4.815897
215.192596	8000.539459	12.123789	-0.045585	4.815884
214.917541	8000.623618	12.128794	-0.045534	4.815910
215.119444	8000.523372	12.133799	-0.045572	4.815880
215.128040	8000.509653	12.138803	-0.045573	4.815876
215.161252	8000.626516	12.143808	-0.045580	4.815910
215.192677	8000.557674	12.148813	-0.045586	4.815889
215.184886	8000.622657	12.153818	-0.045585	4.815908
215.075063	8000.273033	12.158823	-0.045564	4.815807
215.314284	8000.521259	12.163827	-0.045609	4.815878
215.184666	8000.527725	12.168832	-0.045585	4.815881
215.158556	8000.639365	12.173837	-0.045580	4.815913
215.097236	8000.488999	12.178842	-0.045569	4.815870
215.155383	8000.599861	12.183847	-0.045580	4.815902
215.158961	8000.530571	12.188851	-0.045581	4.815882
215.130164	8000.609088	12.193856	-0.045576	4.815905
215.370894	8000.530809	12.198861	-0.045621	4.815881
215.283828	8000.520886	12.203866	-0.045605	4.815878
215.162028	8000.554155	12.208871	-0.045582	4.815888
215.186350	8000.448919	12.213875	-0.045587	4.815857
215.269129	8000.528163	12.218880	-0.045602	4.815880
215.303009	8000.521253	12.223885	-0.045609	4.815878
215.266252	8000.576166	12.228890	-0.045602	4.815894
215.374393	8000.527766	12.233895	-0.045622	4.815880
215.472748	8000.543236	12.238899	-0.045641	4.815884
215.318992	8000.612273	12.243904	-0.045613	4.815905
215.434209	8000.555450	12.248909	-0.045634	4.815887
215.426029	8000.537192	12.253914	-0.045633	4.815882
215.324201	8000.440597	12.258919	-0.045614	4.815854
215.303994	8000.624895	12.263923	-0.045610	4.815908
215.176015	8000.522543	12.268928	-0.045587	4.815879
215.301045	8000.506428	12.273933	-0.045610	4.815874
215.099226	8000.602436	12.278938	-0.045573	4.815903
215.330315	8000.449305	12.283943	-0.045616	4.815857
215.319710	8000.517443	12.288947	-0.045614	4.815877
215.238362	8000.610054	12.293952	-0.045599	4.815904
215.393589	8000.447165	12.298957	-0.045628	4.815856
215.295416	8000.511761	12.303962	-0.045610	4.815875
215.246075	8000.381863	12.308967	-0.045601	4.815838
215.346829	8000.452860	12.313971	-0.045620	4.815858
215.389074	8000.526117	12.318976	-0.045628	4.815879
215.446862	8000.545202	12.323981	-0.045639	4.815884
215.298906	8000.499085	12.328986	-0.045612	4.815872
215.235858	8000.565313	12.333991	-0.045600	4.815891
215.331144	8000.596739	12.338995	-0.045618	4.815900
215.191773	8000.508076	12.344000	-0.045592	4.815875
215.338880	8000.554209	12.349005	-0.045620	4.815887
215.401926	8000.605392	12.354010	-0.045632	4.815902
215.487253	8000.540619	12.359015	-0.045648	4.815883
215.305072	8000.437395	12.364019	-0.045614	4.815853
215.567143	8000.556873	12.369024	-0.045663	4.815887
215.570426	8000.145041	12.374029	-0.045663	4.815767
215.238836	8000.341402	12.379034	-0.045602	4.815826
215.448434	8000.385337	12.384039	-0.045641	4.815838
215.362722	8000.355162	12.389043	-0.045625	4.815829
215.348089	8000.286647	12.394048	-0.045623	4.815809
215.370577	8000.271017	12.399053	-0.045627	4.815804
215.300005	8000.421424	12.404058	-0.045614	4.815849
215.295900	8000.525948	12.409063	-0.045614	4.815879
215.355977	8000.385005	12.414067	-0.045625	4.815838
215.542357	8000.527808	12.419072	-0.045660	4.815879
215.583093	8000.388688	12.424077	-0.045668	4.815838
215.289061	8000.505622	12.429082	-0.045613	4.815873
215.387849	8000.479481	12.434087	-0.045632	4.815865
215.302662	8000.524010	12.439091	-0.045616	4.815879
215.464731	8000.539438	12.444096	-0.045646	4.815882
215.514369	8000.349240	12.449101	-0.045656	4.815827
215.387133	8000.521145	12.454106	-0.045632	4.815877
215.482373	8000.408512	12.459111	-0.045650	4.815844
215.475480	8000.404147	12.464115	-0.045649	4.815843
215.436443	8000.391796	12.469120	-0.045642	4.815839
215.519749	8000.253361	12.474125	-0.045657	4.815798
215.405372	8000.560994	12.479130	-0.045637	4.815889
215.294376	8000.434372	12.484135	-0.045616	4.815853
215.425727	8000.461043	12.489139	-0.045641	4.815860
215.221849	8000.441772	12.494144	-0.045603	4.815855
215.312059	8000.291710	12.499149	-0.045620	4.815811
215.383403	8000.569251	12.504154	-0.045633	4.815892
215.449108	8000.436935	12.509159	-0.045646	4.815853
215.504914	8000.303393	12.514163	-0.045656	4.815813
215.519031	8000.359123	12.519168	-0.045659	4.815829
215.569337	8000.389826	12.524173	-0.045668	4.815838
215.434339	8000.533862	12.529178	-0.045644	4.815881
215.448990	8000.437006	12.534183	-0.045646	4.815853
215.372574	8000.408047	12.539187	-0.045632	4.815844
215.248634	8000.416738	12.544192	-0.045609	4.815848
215.389361	8000.541734	12.549197	-0.045636	4.815883
215.312682	8000.415664	12.554202	-0.045622	4.815847
215.561294	8000.405806	12.559207	-0.045668	4.815843
215.376690	8000.426327	12.564211	-0.045634	4.815850
215.480633	8000.641435	12.569216	-0.045654	4.815912
215.405023	8000.262479	12.574221	-0.045639	4.815802
215.259248	8000.566406	12.579226	-0.045613	4.815891
215.415687	8000.408872	12.584231	-0.045642	4.815844
215.603721	8000.431119	12.589235	-0.045677	4.815850
215.474235	8000.527224	12.594240	-0.045653	4.815879
215.514330	8000.353946	12.599245	-0.045661	4.815828
215.555768	8000.478411	12.604250	-0.045669	4.815864
215.543096	8000.448343	12.609255	-0.045667	4.815855
215.440225	8000.380543	12.614259	-0.045647	4.815836
215.522698	8000.517406	12.619264	-0.045663	4.815876
215.637945	8000.422168	12.624269	-0.045685	4.815847
215.553783	8000.502996	12.629274	-0.045669	4.815871
215.545613	8000.436719	12.634279	-0.045668	4.815852
215.564352	8000.489323	12.639283	-0.045672	4.815867
215.531131	8000.424777	12.644288	-0.045665	4.815848
215.489231	8000.414513	12.649293	-0.045658	4.815846
215.333267	8000.403482	12.654298	-0.045629	4.815843
215.511140	8000.417029	12.659303	-0.045662	4.815846
215.613736	8000.500862	12.664307	-0.045682	4.815870
215.508956	8000.536539	12.669312	-0.045662	4.815881
215.727636	8000.433361	12.674317	-0.045703	4.815850
215.529866	8000.502757	12.679322	-0.045666	4.815871
215.386615	8000.646661	12.684327	-0.045640	4.815914
215.499029	8000.455338	12.689331	-0.045661	4.815857
215.403819	8000.533854	12.694336	-0.045644	4.815881
215.463714	8000.631939	12.699341	-0.045655	4.815909
215.505063	8000.489626	12.704346	-0.045663	4.815867
215.784752	8000.440785	12.709351	-0.045715	4.815852
215.676769	8000.448667	12.714355	-0.045695	4.815855
215.395331	8000.612756	12.719360	-0.045643	4.815904
215.899249	8000.452276	12.724365	-0.045737	4.815855
215.697717	8000.525880	12.729370	-0.045699	4.815877
215.558238	8000.527918	12.734375	-0.045674	4.815878
215.619420	8000.505441	12.739379	-0.045685	4.815872
215.585678	8000.454759	12.744384	-0.045679	4.815857
215.628966	8000.387175	12.749389	-0.045687	4.815837
215.566597	8000.491830	12.754394	-0.045676	4.815868
215.728870	8000.306644	12.759399	-0.045706	4.815813
215.857988	8000.298065	12.764403	-0.045730	4.815810
215.556187	8000.538659	12.769408	-0.045674	4.815882
215.660814	8000.506209	12.774413	-0.045694	4.815872
215.649991	8000.539130	12.779418	-0.045692	4.815881
215.741841	8000.377355	12.784423	-0.045709	4.815833
215.730251	8000.412398	12.789427	-0.045707	4.815844
215.655849	8000.406947	12.794432	-0.045694	4.815843
215.782511	8000.388724	12.799437	-0.045717	4.815837
215.722599	8000.434728	12.804442	-0.045707	4.815850
215.703492	8000.529408	12.809447	-0.045703	4.815878
215.569802	8000.449372	12.814451	-0.045678	4.815855
215.436700	8000.523010	12.819456	-0.045654	4.815877
215.628421	8000.629620	12.824461	-0.045690	4.815908
215.562764	8000.543209	12.829466	-0.045678	4.815883
215.613553	8000.510960	12.834471	-0.045687	4.815873
215.749189	8000.533432	12.839475	-0.045713	4.815879
215.526592	8000.570415	12.844480	-0.045671	4.815891
215.612188	8000.518452	12.849485	-0.045688	4.815875
215.575977	8000.492273	12.854490	-0.045681	4.815868
215.712496	8000.494484	12.859495	-0.045707	4.815868
215.686693	8000.526097	12.864499	-0.045702	4.815877
215.550448	8000.524987	12.869504	-0.045677	4.815877
215.802323	8000.466094	12.874509	-0.045724	4.815859
215.780438	8000.530851	12.879514	-0.045720	4.815878
215.629735	8000.468682	12.884519	-0.045692	4.815861
215.742610	8000.437433	12.889523	-0.045713	4.815851
215.597144	8000.622919	12.894528	-0.045686	4.815906
215.644575	8000.442287	12.899533	-0.045695	4.815853
215.475318	8000.531350	12.904538	-0.045664	4.815880
215.701723	8000.548880	12.909543	-0.045706	4.815884
215.772979	8000.544706	12.914547	-0.045720	4.815882
215.618291	8000.528359	12.919552	-0.045691	4.815878
215.651501	8000.451009	12.924557	-0.045697	4.815855
215.855201	8000.540737	12.929562	-0.045736	4.815881
215.797716	8000.305062	12.934567	-0.045725	4.815812
215.645731	8000.474436	12.939571	-0.045697	4.815862
215.626305	8000.413313	12.944576	-0.045693	4.815844
215.653946	8000.370021	12.949581	-0.045699	4.815832
215.626505	8000.547801	12.954586	-0.045694	4.815884
215.640707	8000.489353	12.959591	-0.045697	4.815867
215.801160	8000.539970	12.964595	-0.045727	4.815881
215.671006	8000.430112	12.969600	-0.045702	4.815849
215.672100	8000.464292	12.974605	-0.045703	4.815859
215.654645	8000.408536	12.979610	-0.045700	4.815843
215.596958	8000.612508	12.984615	-0.045689	4.815903
215.632154	8000.431679	12.989619	-0.045696	4.815850
215.633997	8000.506421	12.994624	-0.045697	4.815872
215.611413	8000.231827	12.999629	-0.045692	4.815791
215.587337	8000.436338	13.004634	-0.045688	4.815851
215.587847	8000.539870	13.009639	-0.045688	4.815882
215.596959	8000.416247	13.014643	-0.045690	4.815845
215.500088	8000.505407	13.019648	-0.045672	4.815872
215.633490	8000.515038	13.024653	-0.045697	4.815874
215.763087	8000.504333	13.029658	-0.045722	4.815870
215.580304	8000.445916	13.034663	-0.045688	4.815854
215.659400	8000.447204	13.039667	-0.045703	4.815854
215.651542	8000.561273	13.044672	-0.045701	4.815887
215.632800	8000.543912	13.049677	-0.045698	4.815882
215.468427	8000.607443	13.054682	-0.045668	4.815902
215.573903	8000.541926	13.059687	-0.045688	4.815882
215.609967	8000.248000	13.064691	-0.045694	4.815796
215.596344	8000.534847	13.069696	-0.045692	4.815880
215.655657	8000.484595	13.074701	-0.045703	4.815865
215.646897	8000.482334	13.079706	-0.045702	4.815864
215.547660	8000.528772	13.084711	-0.045683	4.815878
215.550254	8000.538432	13.089715	-0.045684	4.815881
215.679686	8000.537328	13.094720	-0.045708	4.815880
215.818836	8000.521441	13.099725	-0.045734	4.815875
215.612622	8000.421030	13.104730	-0.045696	4.815847
215.598215	8000.549934	13.109735	-0.045694	4.815884
215.941659	8000.407146	13.114739	-0.045758	4.815841
215.846031	8000.620113	13.119744	-0.045740	4.815904
215.869417	8000.542604	13.124749	-0.045745	4.815881
215.761067	8000.543009	13.129754	-0.045725	4.815882
215.770569	8000.412988	13.134759	-0.045727	4.815843
215.571249	8000.446078	13.139763	-0.045690	4.815854
215.736024	8000.489294	13.144768	-0.045721	4.815866
215.995522	8000.400645	13.149773	-0.045769	4.815839
215.638988	8000.515507	13.154778	-0.045703	4.815874
215.500642	8000.395913	13.159783	-0.045677	4.815840
215.795425	8000.435885	13.164787	-0.045732	4.815850
215.739926	8000.531047	13.169792	-0.045722	4.815878
215.688274	8000.545170	13.174797	-0.045713	4.815882
215.825953	8000.410810	13.179802	-0.045738	4.815843
215.856598	8000.624741	13.184807	-0.045744	4.815905
215.808130	8000.537539	13.189811	-0.045736	4.815880
215.747548	8000.550451	13.194816	-0.045724	4.815884
215.911611	8000.415448	13.199821	-0.045755	4.815843
215.915748	8000.553188	13.204826	-0.045756	4.815884
215.866871	8000.373140	13.209831	-0.045747	4.815831
216.004136	8000.416981	13.214835	-0.045773	4.815843
215.699491	8000.587100	13.219840	-0.045716	4.815895
215.728238	8000.340007	13.224845	-0.045722	4.815822
215.776719	8000.532882	13.229850	-0.045731	4.815878
216.061505	8000.390217	13.234855	-0.045784	4.815835
216.025148	8000.428063	13.239859	-0.045778	4.815847
215.703052	8000.539210	13.244864	-0.045718	4.815881
215.733908	8000.483164	13.249869	-0.045724	4.815864
215.820462	8000.464297	13.254874	-0.045740	4.815858
215.716807	8000.620577	13.259879	-0.045721	4.815904
215.770928	8000.369623	13.264883	-0.045731	4.815831
215.779017	8000.538372	13.269888	-0.045733	4.815880
215.715123	8000.442385	13.274893	-0.045721	4.815852
215.734400	8000.416032	13.279898	-0.045725	4.815844
215.814508	8000.540054	13.284903	-0.045740	4.815880
215.909912	8000.350590	13.289907	-0.045758	4.815824
215.864918	8000.453391	13.294912	-0.045750	4.815855
215.955463	8000.566910	13.299917	-0.045767	4.815887
215.945931	8000.440851	13.304922	-0.045765	4.815851
215.991599	8000.284735	13.309927	-0.045774	4.815805
216.077666	8000.128203	13.314931	-0.045790	4.815759
216.058138	8000.567554	13.319936	-0.045787	4.815887
215.977735	8000.337911	13.324941	-0.045772	4.815820
215.877889	8000.423823	13.329946	-0.045753	4.815846
215.903215	8000.525621	13.334951	-0.045758	4.815876
215.728394	8000.258179	13.339955	-0.045726	4.815798
215.750567	8000.542402	13.344960	-0.045730	4.815881
215.990854	8000.253894	13.349965	-0.045775	4.815796
215.868861	8000.492046	13.354970	-0.045752	4.815866
215.710191	8000.460695	13.359975	-0.045723	4.815857
215.842795	8000.331589	13.364979	-0.045748	4.815819
215.614179	8000.358871	13.369984	-0.045705	4.815828
215.889104	8000.249129	13.374989	-0.045757	4.815795
215.802573	8000.437697	13.379994	-0.045741	4.815850
215.875360	8000.430345	13.384999	-0.045755	4.815848
215.969960	8000.291023	13.390003	-0.045772	4.815807
215.743090	8000.523220	13.395008	-0.045730	4.815876
215.803673	8000.559424	13.400013	-0.045742	4.815886
215.905654	8000.549342	13.405018	-0.045761	4.815882
215.882215	8000.534039	13.410023	-0.045757	4.815878
215.956464	8000.400792	13.415027	-0.045771	4.815839
216.089852	8000.466980	13.420032	-0.045796	4.815857
215.948846	8000.441249	13.425037	-0.045770	4.815851
215.930292	8000.534872	13.430042	-0.045766	4.815878
216.019014	8000.533113	13.435047	-0.045783	4.815877
216.150251	8000.315413	13.440051	-0.045808	4.815813
215.881742	8000.430624	13.445056	-0.045758	4.815848
215.957264	8000.352887	13.450061	-0.045772	4.815825
216.047591	8000.371429	13.455066	-0.045789	4.815830
215.957755	8000.344387	13.460071	-0.045772	4.815822
216.050791	8000.232785	13.465075	-0.045790	4.815789
216.028129	8000.429851	13.470080	-0.045786	4.815847
216.057864	8000.537057	13.475085	-0.045792	4.815878
216.086140	8000.372122	13.480090	-0.045797	4.815830
216.005399	8000.515966	13.485095	-0.045782	4.815872
216.086213	8000.408435	13.490099	-0.045797	4.815840
216.086952	8000.618685	13.495104	-0.045798	4.815902
216.129417	8000.546818	13.500109	-0.045806	4.815881
216.129839	8000.376100	13.505114	-0.045806	4.815831
215.978718	8000.411032	13.510119	-0.045778	4.815842
215.999642	8000.430591	13.515123	-0.045782	4.815847
215.898422	8000.542092	13.520128	-0.045764	4.815880
215.985230	8000.256449	13.525133	-0.045780	4.815796
215.920267	8000.517929	13.530138	-0.045768	4.815873
215.918478	8000.447485	13.535143	-0.045768	4.815853
215.822768	8000.556940	13.540147	-0.045750	4.815885
215.692225	8000.520706	13.545152	-0.045726	4.815875
215.957615	8000.515387	13.550157	-0.045776	4.815872
215.934917	8000.505432	13.555162	-0.045771	4.815869
215.898886	8000.540082	13.560167	-0.045765	4.815880
215.989682	8000.162733	13.565171	-0.045782	4.815769
216.091744	8000.421563	13.570176	-0.045801	4.815844
216.092661	8000.438667	13.575181	-0.045801	4.815849
215.975992	8000.450676	13.580186	-0.045780	4.815853
216.140296	8000.553645	13.585191	-0.045811	4.815882
215.952037	8000.330803	13.590195	-0.045776	4.815818
215.714455	8000.404894	13.595200	-0.045732	4.815841
215.816642	8000.366003	13.600205	-0.045751	4.815829
215.880870	8000.408668	13.605210	-0.045763	4.815841
216.184054	8000.428502	13.610215	-0.045820	4.815846
216.043954	8000.458275	13.615219	-0.045794	4.815855
215.921201	8000.621719	13.620224	-0.045771	4.815903
216.067139	8000.440536	13.625229	-0.045798	4.815850
215.943288	8000.423618	13.630234	-0.045776	4.815845
216.062275	8000.554670	13.635239	-0.045798	4.815883
216.307744	8000.529823	13.640243	-0.045844	4.815875
215.963110	8000.538163	13.645248	-0.045780	4.815879
216.111930	8000.386907	13.650253	-0.045808	4.815834
216.180251	8000.360276	13.655258	-0.045820	4.815826
215.979907	8000.551283	13.660263	-0.045783	4.815882
216.120138	8000.406291	13.665267	-0.045810	4.815839
216.169422	8000.339871	13.670272	-0.045819	4.815820
216.045060	8000.513959	13.675277	-0.045796	4.815871
216.008313	8000.423744	13.680282	-0.045789	4.815845
215.990785	8000.531256	13.685287	-0.045786	4.815877
216.133280	8000.435388	13.690291	-0.045813	4.815848
215.981841	8000.523671	13.695296	-0.045785	4.815874
215.923306	8000.408562	13.700301	-0.045774	4.815841
216.109634	8000.521489	13.705306	-0.045809	4.815873
216.339321	8000.551879	13.710311	-0.045852	4.815881
216.269042	8000.378955	13.715315	-0.045839	4.815831
215.965414	8000.557628	13.720320	-0.045783	4.815884
216.154147	8000.395276	13.725325	-0.045818	4.815836
216.124561	8000.542078	13.730330	-0.045813	4.815879
215.944169	8000.429275	13.735335	-0.045779	4.815847
216.348319	8000.397378	13.740339	-0.045855	4.815836
216.183423	8000.483310	13.745344	-0.045824	4.815862
216.200371	8000.269106	13.750349	-0.045827	4.815799
216.007789	8000.525332	13.755354	-0.045792	4.815875
216.238617	8000.461832	13.760359	-0.045835	4.815855
216.060980	8000.415236	13.765363	-0.045802	4.815842
216.014036	8000.513738	13.770368	-0.045794	4.815871
216.265664	8000.420694	13.775373	-0.045840	4.815843
216.168602	8000.429817	13.780378	-0.045823	4.815846
215.957601	8000.424302	13.785383	-0.045783	4.815845
216.158666	8000.391270	13.790387	-0.045821	4.815835
216.001486	8000.502937	13.795392	-0.045792	4.815868
216.105948	8000.427800	13.800397	-0.045812	4.815846
216.177443	8000.407623	13.805402	-0.045825	4.815839
215.973857	8000.409697	13.810407	-0.045787	4.815841
216.045483	8000.426871	13.815411	-0.045801	4.815846
216.039496	8000.410783	13.820416	-0.045800	4.815841
216.331759	8000.302386	13.825421	-0.045854	4.815808
216.131027	8000.267157	13.830426	-0.045817	4.815798
216.006553	8000.465787	13.835431	-0.045794	4.815857
216.043583	8000.284987	13.840435	-0.045801	4.815804
215.991502	8000.489050	13.845440	-0.045792	4.815864
216.000851	8000.455068	13.850445	-0.045794	4.815854
216.070685	8000.535173	13.855450	-0.045807	4.815877
216.083862	8000.507655	13.860455	-0.045810	4.815869
216.239988	8000.432282	13.865459	-0.045839	4.815846
216.162668	8000.556973	13.870464	-0.045825	4.815883
216.114209	8000.302233	13.875469	-0.045816	4.815809
216.098901	8000.531432	13.880474	-0.045813	4.815876
215.895086	8000.516428	13.885479	-0.045775	4.815872
216.049068	8000.537062	13.890483	-0.045804	4.815878
216.221668	8000.440612	13.895488	-0.045836	4.815849
216.002111	8000.274892	13.900493	-0.045796	4.815801
216.089970	8000.527093	13.905498	-0.045812	4.815875
216.387320	8000.559640	13.910503	-0.045868	4.815883
216.295852	8000.452536	13.915507	-0.045851	4.815852
216.046373	8000.609672	13.920512	-0.045805	4.815899
216.193274	8000.535217	13.925517	-0.045832	4.815877
216.371221	8000.370557	13.930522	-0.045865	4.815828
216.112619	8000.537150	13.935527	-0.045817	4.815877
216.320678	8000.549050	13.940531	-0.045856	4.815880
216.365700	8000.547656	13.945536	-0.045865	4.815879
216.275525	8000.265565	13.950541	-0.045848	4.815797
216.104754	8000.502933	13.955546	-0.045817	4.815867
216.163716	8000.560455	13.960551	-0.045828	4.815884
216.284281	8000.383133	13.965555	-0.045850	4.815832
216.316721	8000.525598	13.970560	-0.045857	4.815873
216.329051	8000.283573	13.975565	-0.045859	4.815802
216.408728	8000.388381	13.980570	-0.045874	4.815833
216.047193	8000.315349	13.985575	-0.045807	4.815813
216.109114	8000.208581	13.990579	-0.045818	4.815781
216.266376	8000.444826	13.995584	-0.045848	4.815850
216.326997	8000.522649	14.000589	-0.045860	4.815872
216.141868	8000.543161	14.005594	-0.045825	4.815879
216.418035	8000.489996	14.010599	-0.045877	4.815862
216.303596	8000.373986	14.015603	-0.045856	4.815829
216.012753	8000.620094	14.020608	-0.045802	4.815902
216.100306	8000.510537	14.025613	-0.045818	4.815870
216.149725	8000.517749	14.030618	-0.045828	4.815872
216.148188	8000.502799	14.035623	-0.045827	4.815867
216.114163	8000.585503	14.040627	-0.045821	4.815892
216.389529	8000.559003	14.045632	-0.045873	4.815882
216.325474	8000.538778	14.050637	-0.045861	4.815877
216.153077	8000.529615	14.055642	-0.045829	4.815875
216.166917	8000.529852	14.060647	-0.045832	4.815875
216.333911	8000.515481	14.065651	-0.045863	4.815870
216.104670	8000.519276	14.070656	-0.045821	4.815872
215.961804	8000.508454	14.075661	-0.045794	4.815870
216.118571	8000.616638	14.080666	-0.045824	4.815901
216.223220	8000.503086	14.085671	-0.045843	4.815867
216.253799	8000.406484	14.090675	-0.045849	4.815838
216.270805	8000.504949	14.095680	-0.045852	4.815867
216.256267	8000.544213	14.100685	-0.045850	4.815879
216.134897	8000.432360	14.105690	-0.045827	4.815847
216.267906	8000.516684	14.110695	-0.045852	4.815871
216.203305	8000.420685	14.115699	-0.045840	4.815843
216.092008	8000.634468	14.120704	-0.045820	4.815906
216.104566	8000.446870	14.125709	-0.045822	4.815851
216.331874	8000.520974	14.130714	-0.045865	4.815872
216.239927	8000.513106	14.135719	-0.045848	4.815870
216.294765	8000.558823	14.140723	-0.045858	4.815883
216.244711	8000.528152	14.145728	-0.045849	4.815874
216.269583	8000.527500	14.150733	-0.045854	4.815874
216.296533	8000.562097	14.155738	-0.045859	4.815884
216.292603	8000.534302	14.160743	-0.045859	4.815876
216.457932	8000.486823	14.165747	-0.045890	4.815861
216.433963	8000.525936	14.170752	-0.045885	4.815872
216.337771	8000.413420	14.175757	-0.045867	4.815840
216.468322	8000.474229	14.180762	-0.045892	4.815857
216.326545	8000.451686	14.185767	-0.045866	4.815851
216.501368	8000.356338	14.190771	-0.045898	4.815823
216.583293	8000.387551	14.195776	-0.045914	4.815831
216.494637	8000.539806	14.200781	-0.045898	4.815876
216.288064	8000.482072	14.205786	-0.045859	4.815860
216.398219	8000.539350	14.210791	-0.045880	4.815877
216.469713	8000.437004	14.215795	-0.045893	4.815846
216.407227	8000.522450	14.220800	-0.045882	4.815872
216.481716	8000.440428	14.225805	-0.045896	4.815847
216.547614	7999.512054	14.230810	-0.045908	4.815575

216.540377	7996.259828	14.235815	-0.045904	4.814624
216.435295	7990.708221	14.240819	-0.045881	4.812999
216.244193	7983.962073	14.245824	-0.045842	4.811025
216.421893	7976.652262	14.250829	-0.045870	4.808883
216.312384	7969.034498	14.255834	-0.045845	4.806651
215.996038	7961.177657	14.260839	-0.045781	4.804349
216.351369	7953.379444	14.265843	-0.045842	4.802060
216.127095	7945.407161	14.270848	-0.045796	4.799721
216.098640	7937.416198	14.275853	-0.045785	4.797375
216.149366	7929.452615	14.280858	-0.045790	4.795035
216.091878	7921.395794	14.285863	-0.045774	4.792668
216.047401	7913.416408	14.290867	-0.045761	4.790321
215.986903	7905.381323	14.295872	-0.045744	4.787958
216.077848	7897.378807	14.300877	-0.045756	4.785602
215.940721	7889.418482	14.305882	-0.045726	4.783258
215.850069	7881.398113	14.310887	-0.045704	4.780895
215.950191	7873.438237	14.315891	-0.045717	4.778549
215.863725	7865.382482	14.320896	-0.045696	4.776173
215.787516	7857.412356	14.325901	-0.045677	4.773822
215.756879	7849.416100	14.330906	-0.045666	4.771461
215.612436	7841.374875	14.335911	-0.045634	4.769086
215.699217	7833.379585	14.340915	-0.045645	4.766723
215.605326	7825.356534	14.345920	-0.045623	4.764352
215.671873	7817.431191	14.350925	-0.045630	4.762007
215.624148	7809.354448	14.355930	-0.045616	4.759617
215.616176	7801.424540	14.360935	-0.045610	4.757269
215.737560	7793.348278	14.365939	-0.045627	4.754876
215.509587	7785.332262	14.370944	-0.045580	4.752501
215.314594	7777.302809	14.375949	-0.045538	4.750120
215.358120	7769.345191	14.380954	-0.045541	4.747759
215.398595	7761.293708	14.385959	-0.045544	4.745369
215.381753	7753.345532	14.390963	-0.045536	4.743008
215.099949	7745.343027	14.395968	-0.045478	4.740631
215.234845	7737.358155	14.400973	-0.045498	4.738257
215.152597	7729.391961	14.405978	-0.045478	4.735887
214.973797	7721.316668	14.410983	-0.045440	4.733485
215.255816	7713.318955	14.415987	-0.045487	4.731103
215.058019	7705.289440	14.420992	-0.045445	4.728711
214.964765	7697.301640	14.425997	-0.045423	4.726331
214.869403	7689.257183	14.431002	-0.045400	4.723932
214.933894	7681.335363	14.436007	-0.045407	4.721568
214.972095	7673.327356	14.441011	-0.045409	4.719178
214.737524	7665.370340	14.446016	-0.045360	4.716802
214.791379	7657.298510	14.451021	-0.045365	4.714390
215.080271	7649.305667	14.456026	-0.045414	4.712000
214.712172	7641.264955	14.461031	-0.045340	4.709595
214.832448	7633.340487	14.466035	-0.045358	4.707224
214.827063	7625.307554	14.471040	-0.045352	4.704818
214.807495	7617.352616	14.476045	-0.045343	4.702435
214.520590	7609.355174	14.481050	-0.045285	4.700039
214.433077	7601.336153	14.486055	-0.045263	4.697634
214.492843	7593.334682	14.491059	-0.045269	4.695234
214.483099	7585.297358	14.496064	-0.045262	4.692821
214.472735	7577.279764	14.501069	-0.045255	4.690413
214.394381	7569.301229	14.506074	-0.045236	4.688016
214.224502	7561.274407	14.511079	-0.045199	4.685603
214.386500	7553.338627	14.516083	-0.045224	4.683215
214.249693	7545.271539	14.521088	-0.045194	4.680787
214.188263	7537.323084	14.526093	-0.045177	4.678394
214.144678	7529.343587	14.531098	-0.045164	4.675990
214.068233	7521.268667	14.536103	-0.045145	4.673556
214.102234	7513.158104	14.541107	-0.045146	4.671110
213.842545	7505.206769	14.546112	-0.045093	4.668711
213.894635	7497.227768	14.551117	-0.045097	4.666302
214.037505	7489.225313	14.556122	-0.045119	4.663885
214.038637	7481.231624	14.561127	-0.045114	4.661469
213.987526	7473.254300	14.566131	-0.045099	4.659057
214.112252	7465.255894	14.571136	-0.045118	4.656637
213.940541	7457.206080	14.576141	-0.045081	4.654201
213.928099	7449.243444	14.581146	-0.045073	4.651789
213.764706	7441.212457	14.586151	-0.045038	4.649356
213.848855	7433.242958	14.591155	-0.045048	4.646940
213.601852	7425.192480	14.596160	-0.044997	4.644498
213.685153	7417.263210	14.601165	-0.045008	4.642092
213.832383	7409.235349	14.606170	-0.045030	4.639654
213.541445	7401.267465	14.611175	-0.044971	4.637234
213.515708	7393.233382	14.616179	-0.044961	4.634792
213.604527	7385.187269	14.621184	-0.044973	4.632345
213.406968	7377.142014	14.626189	-0.044931	4.629897
213.468545	7369.206908	14.631194	-0.044937	4.627481
213.509987	7361.178573	14.636199	-0.044940	4.625035
213.524847	7353.259950	14.641203	-0.044938	4.622622
213.503538	7345.203177	14.646208	-0.044929	4.620165
213.663665	7337.195728	14.651213	-0.044953	4.617722
213.541010	7329.217044	14.656218	-0.044926	4.615287
213.289307	7321.177265	14.661223	-0.044874	4.612831
213.151872	7313.184711	14.666227	-0.044843	4.610389
213.212601	7305.162621	14.671232	-0.044849	4.607936
213.132600	7297.130633	14.676237	-0.044829	4.605479
212.963622	7289.213204	14.681242	-0.044793	4.603056
212.989044	7281.211090	14.686247	-0.044792	4.600606
213.012995	7273.239727	14.691251	-0.044792	4.598163
212.778745	7265.198710	14.696256	-0.044743	4.595698
212.732613	7257.115960	14.701261	-0.044730	4.593219
212.789860	7249.100441	14.706266	-0.044735	4.590759
212.714473	7241.097639	14.711271	-0.044716	4.588302
212.627426	7233.110365	14.716275	-0.044695	4.585848
212.740489	7225.120783	14.721280	-0.044711	4.583392
212.689501	7217.175495	14.726285	-0.044696	4.580949
212.482069	7209.151777	14.731290	-0.044653	4.578479
212.442754	7201.134973	14.736295	-0.044640	4.576011
212.591261	7193.146189	14.741299	-0.044663	4.573550
212.414933	7185.113215	14.746304	-0.044625	4.571074
212.478556	7177.094884	14.751309	-0.044632	4.568602
212.672809	7169.150151	14.756314	-0.044663	4.566151
212.379885	7161.135842	14.761319	-0.044603	4.563676
212.346729	7153.185485	14.766323	-0.044592	4.561220
212.278191	7145.149711	14.771328	-0.044574	4.558737
212.144858	7137.152979	14.776333	-0.044544	4.556264
212.165931	7129.135668	14.781338	-0.044543	4.553783
211.984645	7121.089492	14.786343	-0.044504	4.551292
212.005842	7113.119267	14.791347	-0.044503	4.548824
211.979175	7105.126441	14.796352	-0.044493	4.546347
211.833603	7097.138675	14.801357	-0.044461	4.543870
211.981924	7089.180742	14.806362	-0.044484	4.541401
212.105639	7081.104566	14.811367	-0.044502	4.538895
211.976580	7073.159028	14.816371	-0.044473	4.536427
211.829170	7065.112530	14.821376	-0.044440	4.533926
211.859453	7057.076369	14.826381	-0.044441	4.531427
211.841270	7049.122224	14.831386	-0.044432	4.528953
211.647082	7041.094478	14.836391	-0.044391	4.526454
211.843683	7033.122510	14.841395	-0.044423	4.523971
211.691521	7025.168484	14.846400	-0.044389	4.521493
211.539265	7017.106768	14.851405	-0.044356	4.518979
211.522051	7009.212624	14.856410	-0.044348	4.516516
211.425543	7001.076450	14.861415	-0.044325	4.513976
211.409005	6993.034184	14.866419	-0.044317	4.511465
211.511566	6985.051338	14.871424	-0.044331	4.508971
211.566682	6977.053322	14.876429	-0.044336	4.506470
211.416486	6969.076516	14.881434	-0.044303	4.503974
211.473894	6961.097333	14.886439	-0.044308	4.501477
211.443022	6953.093481	14.891443	-0.044298	4.498970
211.432250	6945.102884	14.896448	-0.044291	4.496467
211.113542	6937.089852	14.901453	-0.044226	4.493953
211.214756	6929.080293	14.906458	-0.044240	4.491441
211.239972	6921.032193	14.911463	-0.044240	4.488915
211.144789	6913.071344	14.916467	-0.044217	4.486415
211.021713	6905.025875	14.921472	-0.044189	4.483886
211.023101	6897.064090	14.926477	-0.044184	4.481383
211.086034	6889.078316	14.931482	-0.044191	4.478871
210.887110	6881.093933	14.936487	-0.044149	4.476357
210.905320	6873.041331	14.941491	-0.044147	4.473821
210.948100	6865.042539	14.946496	-0.044150	4.471301
210.775425	6857.006195	14.951501	-0.044113	4.468766
211.041034	6849.071233	14.956506	-0.044157	4.466264
210.928244	6841.013637	14.961511	-0.044131	4.463720
210.758371	6833.089848	14.966515	-0.044095	4.461217
210.499269	6825.053164	14.971520	-0.044041	4.458676
210.572469	6817.045630	14.976525	-0.044050	4.456145
210.583881	6809.049331	14.981530	-0.044047	4.453615
210.526652	6801.008182	14.986535	-0.044031	4.451069
210.700371	6793.016918	14.991539	-0.044058	4.448539
210.922306	6784.999954	14.996544	-0.044095	4.445999
210.717706	6777.012937	15.001549	-0.044052	4.443466
210.582790	6769.049283	15.006554	-0.044021	4.440938
210.420716	6761.030629	15.011559	-0.043986	4.438392
210.513230	6753.051383	15.016563	-0.043998	4.435858
210.499683	6745.015333	15.021568	-0.043991	4.433304
210.340207	6736.965429	15.026573	-0.043956	4.430743
210.337466	6728.985631	15.031578	-0.043951	4.428204
210.093777	6720.968906	15.036583	-0.043900	4.425651
210.116868	6713.026376	15.041587	-0.043899	4.423120
210.112874	6704.992842	15.046592	-0.043894	4.420560
209.873072	6697.018502	15.051597	-0.043844	4.418015
210.042083	6689.002367	15.056602	-0.043870	4.415458
209.942483	6680.986270	15.061607	-0.043847	4.412898
210.004025	6672.993783	15.066611	-0.043853	4.410345
209.693289	6664.978749	15.071616	-0.043790	4.407781
209.833193	6656.977702	15.076621	-0.043811	4.405223
209.841290	6649.052684	15.081626	-0.043808	4.402686
209.628231	6640.975136	15.086631	-0.043763	4.400099
209.708416	6633.060119	15.091635	-0.043773	4.397563
209.731163	6625.028942	15.096640	-0.043772	4.394988
209.793363	6616.997893	15.101645	-0.043779	4.392412
209.746669	6608.963729	15.106650	-0.043765	4.389833
209.792249	6600.965713	15.111655	-0.043768	4.387265
209.729970	6592.975279	15.116659	-0.043752	4.384696
209.506272	6585.047815	15.121664	-0.043705	4.382146
209.484118	6576.993316	15.126669	-0.043696	4.379554
209.429446	6569.045031	15.131674	-0.043681	4.376995
209.361395	6560.974746	15.136679	-0.043663	4.374395
209.410153	6552.997139	15.141683	-0.043667	4.371824
209.445800	6545.000270	15.146688	-0.043668	4.369246
209.300573	6537.018379	15.151693	-0.043636	4.366669
209.230314	6528.987604	15.156698	-0.043618	4.364076
209.183108	6521.047163	15.161703	-0.043604	4.361510
209.151207	6513.007810	15.166707	-0.043593	4.358911
208.908643	6505.044082	15.171712	-0.043543	4.356333
208.955805	6496.960685	15.176717	-0.043547	4.353717
208.919973	6488.906964	15.181722	-0.043535	4.351109
208.729645	6480.876698	15.186727	-0.043495	4.348506
208.862054	6472.913898	15.191731	-0.043514	4.345925
208.984228	6464.963694	15.196736	-0.043532	4.343346
208.939820	6456.994790	15.201741	-0.043519	4.340759
208.700177	6448.989688	15.206746	-0.043469	4.338157
208.850860	6440.978166	15.211751	-0.043492	4.335554
208.762500	6432.976620	15.216755	-0.043471	4.332951
208.531891	6424.950448	15.221760	-0.043423	4.330338
208.492416	6416.964276	15.226765	-0.043410	4.327737
208.505418	6408.970255	15.231770	-0.043408	4.325133
208.411141	6400.952841	15.236775	-0.043385	4.322519
208.489114	6392.981365	15.241779	-0.043394	4.319919
208.662647	6385.005774	15.246784	-0.043422	4.317317
208.397763	6376.959084	15.251789	-0.043367	4.314687
208.409864	6368.960603	15.256794	-0.043365	4.312073
208.401854	6360.884409	15.261799	-0.043358	4.309432
208.524842	6352.956009	15.266803	-0.043376	4.306839
208.258277	6344.940623	15.271808	-0.043321	4.304213
208.247597	6336.968842	15.276813	-0.043314	4.301601
208.271880	6328.992493	15.281818	-0.043314	4.298987
208.019913	6320.938326	15.286823	-0.043262	4.296343
207.967510	6312.948005	15.291827	-0.043247	4.293721
208.016913	6304.898282	15.296832	-0.043251	4.291078
207.957131	6296.898040	15.301837	-0.043235	4.288448
208.178911	6288.947817	15.306842	-0.043271	4.285836
208.172126	6280.940835	15.311847	-0.043265	4.283202
208.095406	6272.959548	15.316851	-0.043246	4.280574
207.916809	6264.953624	15.321856	-0.043207	4.277935
207.777443	6256.936546	15.326861	-0.043176	4.275291
207.897671	6248.883602	15.331866	-0.043194	4.272636
207.778698	6240.833444	15.336871	-0.043166	4.269978
207.776920	6232.908093	15.341875	-0.043161	4.267361
207.829767	6224.854855	15.346880	-0.043166	4.264701
207.690409	6216.947757	15.351885	-0.043135	4.262085
207.485690	6208.897362	15.356890	-0.043092	4.259420
207.355600	6200.969780	15.361895	-0.043062	4.256794
207.398397	6192.935904	15.366899	-0.043065	4.254133
207.533764	6184.913885	15.371904	-0.043085	4.251476
207.230838	6176.920409	15.376909	-0.043024	4.248822
207.505067	6168.947747	15.381914	-0.043070	4.246178
207.331998	6160.919347	15.386919	-0.043033	4.243510
207.351319	6152.983554	15.391923	-0.043031	4.240874
207.337297	6144.948528	15.396928	-0.043024	4.238202
207.288556	6136.952421	15.401933	-0.043010	4.235541
207.137519	6128.939039	15.406938	-0.042976	4.232872
207.171486	6120.905672	15.411943	-0.042978	4.230196
207.191526	6112.929288	15.416947	-0.042976	4.227537
207.128418	6104.951040	15.421952	-0.042960	4.224875
207.001595	6096.973215	15.426957	-0.042931	4.222211
207.031751	6088.958371	15.431962	-0.042931	4.219535
206.940011	6080.971919	15.436967	-0.042909	4.216865
207.027666	6072.929093	15.441971	-0.042921	4.214176
206.657585	6064.967929	15.446976	-0.042847	4.211508
206.769265	6056.894538	15.451981	-0.042862	4.208806
206.657889	6048.986933	15.456986	-0.042837	4.206156
206.602999	6040.951337	15.461991	-0.042821	4.203461
206.794842	6032.976413	15.466995	-0.042852	4.200788
206.817152	6024.995132	15.472000	-0.042851	4.198109
206.721585	6016.934436	15.477005	-0.042828	4.195400
206.638056	6008.885106	15.482010	-0.042808	4.192694
206.511367	6000.794157	15.487015	-0.042779	4.189971
206.427340	5992.887040	15.492019	-0.042758	4.187309
206.491621	5984.868014	15.497024	-0.042765	4.184609
206.453086	5976.935318	15.502029	-0.042753	4.181935
206.507293	5968.957450	15.507034	-0.042758	4.179246
206.270606	5960.953677	15.512039	-0.042709	4.176542
206.320514	5952.931741	15.517043	-0.042713	4.173834
206.175079	5944.919721	15.522048	-0.042681	4.171126
206.160703	5936.880845	15.527053	-0.042673	4.168407
206.175386	5928.915427	15.532058	-0.042671	4.165713
206.278218	5920.944772	15.537063	-0.042685	4.163016
206.087531	5912.942359	15.542067	-0.042645	4.160303
206.063860	5904.946838	15.547072	-0.042635	4.157592
206.135175	5896.894356	15.552077	-0.042643	4.154862
206.176877	5888.918984	15.557082	-0.042646	4.152155
206.088606	5880.884457	15.562087	-0.042625	4.149425
206.037098	5872.900793	15.567091	-0.042610	4.146711
205.874488	5864.907981	15.572096	-0.042575	4.143991
205.630550	5856.902308	15.577101	-0.042524	4.141264
205.861234	5848.938106	15.582106	-0.042562	4.138555
205.920570	5840.887227	15.587111	-0.042568	4.135812
205.809940	5832.923816	15.592115	-0.042542	4.133095
205.481789	5824.869368	15.597120	-0.042476	4.130343
205.467401	5816.901227	15.602125	-0.042469	4.127622
205.642453	5808.888425	15.607130	-0.042496	4.124886
205.380197	5800.914450	15.612135	-0.042442	4.122157
205.269492	5792.897342	15.617139	-0.042417	4.119413
205.668689	5784.954023	15.622144	-0.042486	4.116698
205.499686	5776.901460	15.627149	-0.042449	4.113938
205.371506	5768.914742	15.632154	-0.042420	4.111198
205.275031	5760.843949	15.637159	-0.042397	4.108428
205.342178	5752.874212	15.642163	-0.042405	4.105693
205.137085	5744.908426	15.647168	-0.042362	4.102954
205.093187	5736.920935	15.652173	-0.042348	4.100208
205.294673	5728.945618	15.657178	-0.042381	4.097468
205.014329	5720.907328	15.662183	-0.042324	4.094697
204.996861	5712.898718	15.667187	-0.042315	4.091939
204.923096	5704.881444	15.672192	-0.042297	4.089174
204.739405	5696.923755	15.677197	-0.042257	4.086427
204.865612	5688.943785	15.682202	-0.042276	4.083675
204.930309	5680.918295	15.687207	-0.042283	4.080904
204.936750	5672.987272	15.692211	-0.042279	4.078163
204.774748	5664.985365	15.697216	-0.042244	4.075394
204.579698	5656.956945	15.702221	-0.042202	4.072613
204.853951	5648.917658	15.707226	-0.042248	4.069833
204.750515	5640.927155	15.712231	-0.042224	4.067062
204.634009	5632.905785	15.717235	-0.042197	4.064279
204.649144	5624.983450	15.722240	-0.042195	4.061530
204.600222	5616.934328	15.727245	-0.042181	4.058734
204.513436	5608.992053	15.732250	-0.042160	4.055973
204.324964	5600.948203	15.737255	-0.042120	4.053173
204.481814	5592.903515	15.742259	-0.042144	4.050376
204.331415	5584.940073	15.747264	-0.042111	4.047601
204.205057	5576.904113	15.752269	-0.042082	4.044799
204.379282	5569.007725	15.757274	-0.042110	4.042048
204.264419	5560.951063	15.762279	-0.042083	4.039236
204.156136	5552.998102	15.767283	-0.042058	4.036457
204.126043	5544.906161	15.772288	-0.042047	4.033629
204.031060	5536.836126	15.777293	-0.042025	4.030806
203.991775	5528.885307	15.782298	-0.042012	4.028023
203.822592	5520.846772	15.787303	-0.041976	4.025206
203.884372	5512.928456	15.792307	-0.041982	4.022432
203.878453	5504.913553	15.797312	-0.041976	4.019622
203.714551	5496.953093	15.802317	-0.041940	4.016826
203.797468	5488.946342	15.807322	-0.041951	4.014016
203.742488	5480.898952	15.812327	-0.041936	4.011187
203.614472	5472.895173	15.817331	-0.041907	4.008371
203.581463	5464.895443	15.822336	-0.041895	4.005556
203.598604	5456.938963	15.827341	-0.041894	4.002754
203.613996	5448.958019	15.832346	-0.041891	3.999942
203.520159	5440.949635	15.837351	-0.041869	3.997117
203.629088	5432.943820	15.842355	-0.041884	3.994294
203.631835	5424.937928	15.847360	-0.041880	3.991467
203.382480	5416.915850	15.852365	-0.041828	3.988628
203.398899	5408.941047	15.857370	-0.041826	3.985808
203.456105	5400.922355	15.862375	-0.041832	3.982971
203.378002	5392.954492	15.867379	-0.041812	3.980149
203.411952	5384.963257	15.872384	-0.041814	3.977317
203.142903	5376.939255	15.877389	-0.041758	3.974467
203.151689	5368.951885	15.882394	-0.041755	3.971633
202.999517	5360.911121	15.887399	-0.041722	3.968774
203.123224	5352.956951	15.892403	-0.041740	3.965950
202.942167	5344.980078	15.897408	-0.041701	3.963110
202.844033	5336.971676	15.902413	-0.041678	3.960258
203.069933	5329.026970	15.907418	-0.041715	3.957432
202.772177	5320.978520	15.912423	-0.041654	3.954558
202.884964	5312.948344	15.917427	-0.041670	3.951696
202.728734	5304.944152	15.922432	-0.041636	3.948836
202.629446	5296.947392	15.927437	-0.041612	3.945978
202.611154	5289.020564	15.932442	-0.041604	3.943144
202.684441	5281.003293	15.937447	-0.041613	3.940277
202.865991	5273.027407	15.942451	-0.041641	3.937425
202.499621	5265.005389	15.947456	-0.041568	3.934545
202.508775	5256.976625	15.952461	-0.041565	3.931667
202.578723	5248.977641	15.957466	-0.041573	3.928798
202.437996	5241.009056	15.962471	-0.041541	3.925935
202.289067	5233.014629	15.967475	-0.041509	3.923060
202.416530	5224.990326	15.972480	-0.041527	3.920177
202.514492	5217.034103	15.977485	-0.041541	3.917316
202.275859	5209.043765	15.982490	-0.041491	3.914434
202.342952	5200.999469	15.987495	-0.041498	3.911537
202.366310	5192.965973	15.992499	-0.041498	3.908640
202.113648	5185.008995	15.997504	-0.041446	3.905764
201.921644	5177.034950	16.002509	-0.041405	3.902881
202.090523	5169.034162	16.007514	-0.041431	3.899992
202.039127	5161.025798	16.012519	-0.041417	3.897095
202.203884	5152.982694	16.017523	-0.041442	3.894186
202.106447	5145.014565	16.022528	-0.041419	3.891298
201.979492	5136.999730	16.027533	-0.041390	3.888390
201.884462	5128.987528	16.032538	-0.041368	3.885482
201.715747	5121.002511	16.037543	-0.041331	3.882580
201.768491	5113.023665	16.042547	-0.041336	3.879682
201.687876	5105.081133	16.047552	-0.041316	3.876792
201.526116	5096.968843	16.052557	-0.041281	3.873837
201.645166	5088.788427	16.057562	-0.041298	3.870861
201.459817	5080.855225	16.062567	-0.041258	3.867966
201.537691	5072.889682	16.067571	-0.041268	3.865063
201.650801	5064.980323	16.072576	-0.041284	3.862178
201.522132	5056.953444	16.077581	-0.041255	3.859244
201.604289	5049.021820	16.082586	-0.041265	3.856346
201.433663	5041.013750	16.087591	-0.041228	3.853414
201.495287	5033.001481	16.092595	-0.041235	3.850482
201.325997	5024.993716	16.097600	-0.041198	3.847545
201.038117	5016.990283	16.102605	-0.041139	3.844604
201.291091	5009.064736	16.107610	-0.041182	3.841701
201.141868	5001.049649	16.112615	-0.041149	3.838755
201.105638	4993.060710	16.117619	-0.041137	3.835819
201.142776	4985.034707	16.122624	-0.041139	3.832868
201.213871	4977.029896	16.127629	-0.041147	3.829923
201.233342	4969.077383	16.132634	-0.041146	3.826994
201.045824	4961.037860	16.137639	-0.041106	3.824027
201.139118	4953.097615	16.142643	-0.041118	3.821100
201.200473	4945.079890	16.147648	-0.041124	3.818141
200.880017	4937.091350	16.152653	-0.041060	3.815183
200.932347	4929.103493	16.157658	-0.041064	3.812230
201.016344	4921.049960	16.162663	-0.041075	3.809252
200.907491	4913.091521	16.167667	-0.041050	3.806302
200.816413	4905.125629	16.172672	-0.041028	3.803348
200.776028	4897.107452	16.177677	-0.041015	3.800373
200.630887	4889.157262	16.182682	-0.040983	3.797418
200.592259	4881.108720	16.187687	-0.040971	3.794427
200.611892	4873.068952	16.192691	-0.040969	3.791439
200.611894	4865.057663	16.197696	-0.040964	3.788458
200.431036	4857.080287	16.202701	-0.040926	3.785483
200.447817	4849.114129	16.207706	-0.040924	3.782515
200.282473	4841.094088	16.212711	-0.040888	3.779520
200.225175	4833.114074	16.217715	-0.040872	3.776540
200.258407	4825.092287	16.222720	-0.040873	3.773544
200.169710	4817.085959	16.227725	-0.040852	3.770549
200.135651	4809.124402	16.232730	-0.040840	3.767569
199.957814	4801.054633	16.237735	-0.040802	3.764543
199.917167	4793.156209	16.242739	-0.040790	3.761582
199.964857	4785.150409	16.247744	-0.040793	3.758581
199.970788	4777.129462	16.252749	-0.040790	3.755570
200.080540	4769.131767	16.257754	-0.040805	3.752569
200.081650	4761.088258	16.262759	-0.040800	3.749545
200.008990	4753.107274	16.267763	-0.040781	3.746540
199.750695	4745.139386	16.272768	-0.040728	3.743533
199.712054	4737.131921	16.277773	-0.040716	3.740515
199.918975	4729.164281	16.282778	-0.040750	3.737515
199.642704	4721.156618	16.287783	-0.040693	3.734485
199.636418	4713.171499	16.292787	-0.040687	3.731469
199.657274	4705.156454	16.297792	-0.040686	3.728439
199.513261	4697.138647	16.302797	-0.040654	3.725401
199.606262	4689.218581	16.307802	-0.040666	3.722404
199.475174	4681.157038	16.312807	-0.040637	3.719345
199.435214	4673.241941	16.317811	-0.040624	3.716342
199.341501	4665.183017	16.322816	-0.040602	3.713280
199.274927	4657.091247	16.327821	-0.040584	3.710204
199.523661	4649.157259	16.332826	-0.040626	3.707193
199.341875	4641.152704	16.337831	-0.040587	3.704143
199.072331	4633.240038	16.342835	-0.040532	3.701122
199.340096	4625.190678	16.347840	-0.040576	3.698060
199.095658	4617.215897	16.352845	-0.040526	3.695012
199.126927	4609.227182	16.357850	-0.040527	3.691962
198.913492	4601.219592	16.362855	-0.040482	3.688897
198.953499	4593.223166	16.367859	-0.040484	3.685839
199.022021	4585.246141	16.372864	-0.040492	3.682787
198.865182	4577.236159	16.377869	-0.040458	3.679715
198.927839	4569.306973	16.382874	-0.040464	3.676676
198.700008	4561.265562	16.387879	-0.040417	3.673584
198.604881	4553.239975	16.392883	-0.040394	3.670500
198.635329	4545.242747	16.397888	-0.040395	3.667426
198.652063	4537.207718	16.402893	-0.040393	3.664335
198.613467	4529.281290	16.407898	-0.040381	3.661282
198.715407	4521.217504	16.412903	-0.040394	3.658178
198.685516	4513.281179	16.417907	-0.040384	3.655116
198.520838	4505.287990	16.422912	-0.040348	3.652026
198.210556	4497.270443	16.427917	-0.040285	3.648920
198.548512	4489.260442	16.432922	-0.040343	3.645832
198.521710	4481.250006	16.437927	-0.040333	3.642731
198.235978	4473.303002	16.442931	-0.040275	3.639645
198.472412	4465.342728	16.447936	-0.040314	3.636566
198.412081	4457.297149	16.452941	-0.040298	3.633443
198.317166	4449.267363	16.457946	-0.040275	3.630322
198.045241	4441.286627	16.462951	-0.040219	3.627213
198.182057	4433.269734	16.467955	-0.040240	3.624098
198.074736	4425.344990	16.472960	-0.040215	3.621010
197.813957	4417.334579	16.477965	-0.040161	3.617881
198.207156	4409.327351	16.482970	-0.040229	3.614769
197.771020	4401.331330	16.487975	-0.040143	3.611636
197.856955	4393.304506	16.492979	-0.040154	3.608502
197.912921	4385.348210	16.497984	-0.040159	3.605393
197.720982	4377.370244	16.502989	-0.040119	3.602265
197.790927	4369.379717	16.507994	-0.040127	3.599137
197.775615	4361.406223	16.512999	-0.040119	3.596011
197.674483	4353.382239	16.518003	-0.040095	3.592859
197.658728	4345.363147	16.523008	-0.040087	3.589710
197.380381	4337.401899	16.528013	-0.040030	3.586572
197.699864	4329.400323	16.533018	-0.040084	3.583433
197.489109	4321.405434	16.538023	-0.040040	3.580279
197.498215	4313.442797	16.543027	-0.040037	3.577141
197.265216	4305.455839	16.548032	-0.039988	3.573984
197.289193	4297.383664	16.553037	-0.039988	3.570798
197.337749	4289.418747	16.558042	-0.039992	3.567652
197.065810	4281.426913	16.563047	-0.039936	3.564483
197.086730	4273.464773	16.568051	-0.039935	3.561332
197.036927	4265.476334	16.573056	-0.039921	3.558165
197.039076	4257.439233	16.578061	-0.039916	3.554978
197.133337	4249.357658	16.583066	-0.039928	3.551773
196.789626	4241.366380	16.588071	-0.039859	3.548588
196.843991	4233.380827	16.593075	-0.039864	3.545414
196.867123	4225.426708	16.598080	-0.039864	3.542249
196.868560	4217.421010	16.603085	-0.039859	3.539059
196.805082	4209.473616	16.608090	-0.039842	3.535889
196.719283	4201.436552	16.613095	-0.039821	3.532679
196.798035	4193.403710	16.618099	-0.039831	3.529472
196.634039	4185.469995	16.623104	-0.039795	3.526295
196.517968	4177.485263	16.628109	-0.039769	3.523097
196.694159	4169.502605	16.633114	-0.039796	3.519905
196.560657	4161.516634	16.638119	-0.039766	3.516699
196.527766	4153.517048	16.643123	-0.039755	3.513488
196.582059	4145.503307	16.648128	-0.039760	3.510271
196.512381	4137.486298	16.653133	-0.039742	3.507046
196.503081	4129.509244	16.658138	-0.039735	3.503836
196.479711	4121.525107	16.663143	-0.039726	3.500620
196.588873	4113.561220	16.668147	-0.039741	3.497413
196.686345	4105.557556	16.673152	-0.039755	3.494187
196.371055	4097.571153	16.678157	-0.039691	3.490951
196.513730	4089.583378	16.683162	-0.039712	3.487727
196.147775	4081.577393	16.688167	-0.039639	3.484476
196.301180	4073.618992	16.693171	-0.039663	3.481258
196.118233	4065.672925	16.698176	-0.039624	3.478031
196.189017	4057.603461	16.703181	-0.039632	3.474759
196.155275	4049.607503	16.708186	-0.039620	3.471511
195.950027	4041.599700	16.713191	-0.039577	3.468249
195.942737	4033.602131	16.718195	-0.039571	3.464994
195.984094	4025.657993	16.723200	-0.039573	3.461760
195.820782	4017.645062	16.728205	-0.039538	3.458488
195.744452	4009.687095	16.733210	-0.039519	3.455239
195.825375	4001.613959	16.738215	-0.039529	3.451944
195.757097	3993.634593	16.743219	-0.039511	3.448680
195.734619	3985.653771	16.748224	-0.039502	3.445413
195.544358	3977.664443	16.753229	-0.039461	3.442134
195.501749	3969.682982	16.758234	-0.039448	3.438861
195.476182	3961.694067	16.763239	-0.039438	3.435581
195.400416	3953.679679	16.768243	-0.039419	3.432287
195.639912	3945.682854	16.773248	-0.039459	3.429007
195.539806	3937.672950	16.778253	-0.039435	3.425707
195.474240	3929.723267	16.783258	-0.039418	3.422430
195.278198	3921.727680	16.788263	-0.039376	3.419126
195.287138	3913.778901	16.793267	-0.039373	3.415845
195.174840	3905.756425	16.798272	-0.039347	3.412527
195.085318	3897.716525	16.803277	-0.039325	3.409199
195.131458	3889.779505	16.808282	-0.039329	3.405915
195.162231	3881.786641	16.813287	-0.039330	3.402604
195.101177	3873.801711	16.818291	-0.039313	3.399290
195.113842	3865.832695	16.823296	-0.039311	3.395982
194.922908	3857.747402	16.828301	-0.039270	3.392615
194.827712	3849.741672	16.833306	-0.039247	3.389281
194.826621	3841.747157	16.838311	-0.039242	3.385952
194.671911	3833.810201	16.843315	-0.039208	3.382639
194.660043	3825.821858	16.848320	-0.039201	3.379305
194.771226	3817.827205	16.853325	-0.039216	3.375970
194.775105	3809.834623	16.858330	-0.039212	3.372629
194.624298	3801.808000	16.863335	-0.039179	3.369265
194.542354	3793.848382	16.868339	-0.039159	3.365928
194.682907	3785.860486	16.873344	-0.039180	3.362584
194.514449	3777.850555	16.878349	-0.039143	3.359216
194.442386	3769.931039	16.883354	-0.039125	3.355886
194.478770	3761.895789	16.888359	-0.039127	3.352508
194.584276	3753.857450	16.893363	-0.039141	3.349127
194.412648	3745.922319	16.898368	-0.039104	3.345777
194.346218	3737.920235	16.903373	-0.039087	3.342399
194.321866	3729.924824	16.908378	-0.039077	3.339022
194.385103	3721.926911	16.913383	-0.039084	3.335644
194.226451	3713.941019	16.918387	-0.039050	3.332259
194.450049	3705.943034	16.923392	-0.039086	3.328880
194.228702	3697.953933	16.928397	-0.039040	3.325484
194.059315	3690.007487	16.933402	-0.039003	3.322105
194.084405	3682.002821	16.938407	-0.039003	3.318705
193.981502	3674.039692	16.943411	-0.038979	3.315315
193.985621	3666.001238	16.948416	-0.038974	3.311893
193.727565	3658.002461	16.953421	-0.038921	3.308474
193.820300	3649.997641	16.958426	-0.038934	3.305063
193.704998	3642.043737	16.963431	-0.038907	3.301662
193.472755	3634.065489	16.968435	-0.038859	3.298242
193.611964	3626.087103	16.973440	-0.038880	3.294833
193.726361	3618.049944	16.978445	-0.038896	3.291395
193.522379	3610.065820	16.983450	-0.038853	3.287963
193.577292	3602.069670	16.988455	-0.038858	3.284533
193.499177	3594.109133	16.993459	-0.038839	3.281109
193.647219	3586.133543	16.998464	-0.038861	3.277684
193.400255	3578.128199	17.003469	-0.038810	3.274227
193.558488	3570.107571	17.008474	-0.038834	3.270775
193.281342	3562.140120	17.013479	-0.038778	3.267326
193.302813	3554.136581	17.018483	-0.038777	3.263869
193.309049	3546.166721	17.023488	-0.038773	3.260423
193.213216	3538.182226	17.028493	-0.038750	3.256962
193.245617	3530.177187	17.033498	-0.038751	3.253495
193.018323	3522.169373	17.038503	-0.038704	3.250011
193.099641	3514.211433	17.043507	-0.038714	3.246558
193.203848	3506.222485	17.048512	-0.038728	3.243089
193.045964	3498.234093	17.053517	-0.038694	3.239606
193.081592	3490.276486	17.058522	-0.038695	3.236140
192.831689	3482.227370	17.063527	-0.038644	3.232619
192.641881	3474.205835	17.068531	-0.038603	3.229109
192.685847	3466.234777	17.073536	-0.038607	3.225626
192.685001	3458.245136	17.078541	-0.038601	3.222130
192.637137	3450.279272	17.083546	-0.038587	3.218638
192.592034	3442.310434	17.088551	-0.038574	3.215142
192.689920	3434.278525	17.093555	-0.038587	3.211619
192.755616	3426.296761	17.098560	-0.038594	3.208114
192.545224	3418.306583	17.103565	-0.038550	3.204590
192.632504	3410.359386	17.108570	-0.038561	3.201093
192.540467	3402.372081	17.113575	-0.038539	3.197567
192.278311	3394.384399	17.118579	-0.038485	3.194029
192.283588	3386.378044	17.123584	-0.038481	3.190491
192.352286	3378.373092	17.128589	-0.038489	3.186952
192.365211	3370.393619	17.133594	-0.038486	3.183419
192.257078	3362.427595	17.138599	-0.038461	3.179882
192.246800	3354.449122	17.143603	-0.038454	3.176340
192.416944	3346.438987	17.148608	-0.038481	3.172787
191.926517	3338.426540	17.153613	-0.038385	3.169201
192.099411	3330.461450	17.158618	-0.038412	3.165661
192.248797	3322.453589	17.163623	-0.038434	3.162096
192.081608	3314.500141	17.168627	-0.038398	3.158539
191.868752	3306.555302	17.173632	-0.038354	3.154979
191.791689	3298.503774	17.178637	-0.038334	3.151373
191.830724	3290.496816	17.183642	-0.038336	3.147788
191.700608	3282.516930	17.188647	-0.038307	3.144203
191.681543	3274.563801	17.193651	-0.038299	3.140632
191.790526	3266.580061	17.198656	-0.038314	3.137048
191.660855	3258.588701	17.203661	-0.038285	3.133446
191.654726	3250.559074	17.208666	-0.038279	3.129828
191.686784	3242.595834	17.213671	-0.038279	3.126238
191.450844	3234.640661	17.218675	-0.038231	3.122635
191.485337	3226.658951	17.223680	-0.038232	3.119028
191.348943	3218.672447	17.228685	-0.038201	3.115407
191.511470	3210.667553	17.233690	-0.038227	3.111787
191.241007	3202.691776	17.238695	-0.038171	3.108157
191.365462	3194.670118	17.243699	-0.038189	3.104519
191.439113	3186.724652	17.248704	-0.038198	3.100909
191.412617	3178.712799	17.253709	-0.038188	3.097261
191.348565	3170.738827	17.258714	-0.038171	3.093623
191.191565	3162.741254	17.263719	-0.038137	3.089967
191.206021	3154.735899	17.268723	-0.038135	3.086310
191.152238	3146.791956	17.273728	-0.038120	3.082674
190.908908	3138.796255	17.278733	-0.038069	3.079001
191.265048	3130.804397	17.283738	-0.038130	3.075353
191.018430	3122.756136	17.288743	-0.038079	3.071647
190.821265	3114.789380	17.293747	-0.038038	3.067976
190.789470	3106.813319	17.298752	-0.038027	3.064304
190.681610	3098.851919	17.303757	-0.038002	3.060631
190.729888	3090.872610	17.308762	-0.038006	3.056953
190.668947	3082.874252	17.313767	-0.037989	3.053256
190.607103	3074.860740	17.318771	-0.037973	3.049548
190.701261	3066.931892	17.323776	-0.037985	3.045881
190.526602	3058.934656	17.328781	-0.037948	3.042166
190.596824	3050.954857	17.333786	-0.037956	3.038466
190.610369	3042.959064	17.338791	-0.037953	3.034752
190.523396	3034.958022	17.343795	-0.037932	3.031025
190.496351	3027.002154	17.348800	-0.037922	3.027318
190.102759	3019.036763	17.353805	-0.037844	3.023584
190.219592	3011.048094	17.358810	-0.037860	3.019860
190.293609	3003.069036	17.363815	-0.037869	3.016133
190.233250	2995.050583	17.368819	-0.037853	3.012377
190.097079	2987.067444	17.373824	-0.037822	3.008628
189.947425	2979.093085	17.378829	-0.037789	3.004879
190.187648	2971.128125	17.383834	-0.037829	3.001148
190.090670	2963.156197	17.388839	-0.037806	2.997393
190.009326	2955.156225	17.393843	-0.037786	2.993621
190.020349	2947.151288	17.398848	-0.037783	2.989846
189.930626	2939.161218	17.403853	-0.037761	2.986068
189.812745	2931.203441	17.408858	-0.037734	2.982300
189.784277	2923.208682	17.413863	-0.037724	2.978514
189.893934	2915.211977	17.418867	-0.037739	2.974728
189.647428	2907.258923	17.423872	-0.037688	2.970941
189.660307	2899.258778	17.428877	-0.037686	2.967140
189.716161	2891.274752	17.433882	-0.037691	2.963343
189.438961	2883.311240	17.438887	-0.037634	2.959535
189.485052	2875.361849	17.443891	-0.037638	2.955745
189.475804	2867.347620	17.448896	-0.037631	2.951916
189.246205	2859.354596	17.453901	-0.037583	2.948081
189.201475	2851.387880	17.458906	-0.037570	2.944263
189.216901	2843.419784	17.463911	-0.037568	2.940443
189.023002	2835.436730	17.468915	-0.037527	2.936599
189.157942	2827.439421	17.473920	-0.037547	2.932761
189.111215	2819.429576	17.478925	-0.037533	2.928902
189.268286	2811.441675	17.483930	-0.037557	2.925060
189.068219	2803.499439	17.488935	-0.037515	2.921215
189.002855	2795.521998	17.493939	-0.037498	2.917356
189.090829	2787.515083	17.498944	-0.037509	2.913485
188.851786	2779.447276	17.503949	-0.037460	2.909562
188.792251	2771.507603	17.508954	-0.037443	2.905706
188.961148	2763.516657	17.513959	-0.037470	2.901832
188.860830	2755.563537	17.518963	-0.037446	2.897956
188.726277	2747.612100	17.523968	-0.037416	2.894075
188.520216	2739.604534	17.528973	-0.037373	2.890157
188.532921	2731.646806	17.533978	-0.037370	2.886270
188.486795	2723.674465	17.538983	-0.037356	2.882367
188.429252	2715.708490	17.543987	-0.037341	2.878461
188.481321	2707.731554	17.548992	-0.037345	2.874551
188.408938	2699.705085	17.553997	-0.037327	2.870604
188.307353	2691.746882	17.559002	-0.037303	2.866684
188.260689	2683.775075	17.564007	-0.037289	2.862754
188.287538	2675.776862	17.569011	-0.037289	2.858811
188.369263	2667.815059	17.574016	-0.037299	2.854883
188.189169	2659.817445	17.579021	-0.037261	2.850917
188.407217	2651.836994	17.584026	-0.037296	2.846976
188.303181	2643.887022	17.589031	-0.037272	2.843027
188.055889	2635.915435	17.594035	-0.037221	2.839054
187.966342	2627.964787	17.599040	-0.037199	2.835094
187.883437	2619.935596	17.604045	-0.037179	2.831090
187.840659	2611.953880	17.609050	-0.037166	2.827106
187.801842	2603.959251	17.614055	-0.037153	2.823111
187.937827	2595.970275	17.619059	-0.037174	2.819122
187.865063	2588.026454	17.624064	-0.037155	2.815139
187.601819	2580.039317	17.629069	-0.037101	2.811117
187.695698	2572.044364	17.634074	-0.037114	2.807107
187.920403	2564.074221	17.639079	-0.037150	2.803110
187.686732	2556.114406	17.644083	-0.037102	2.799086
187.832526	2548.156257	17.649088	-0.037124	2.795080
187.628889	2540.156090	17.654093	-0.037081	2.791026
187.444573	2532.185761	17.659098	-0.037042	2.786982
187.578488	2524.193163	17.664103	-0.037062	2.782940
187.400588	2516.223839	17.669107	-0.037023	2.778886
187.531764	2508.254116	17.674112	-0.037043	2.774843
187.336981	2500.265380	17.679117	-0.037002	2.770766
187.360820	2492.307594	17.684122	-0.037001	2.766712
187.244663	2484.339984	17.689127	-0.036974	2.762638
186.915233	2476.396428	17.694131	-0.036908	2.758557
187.044705	2468.412029	17.699136	-0.036927	2.754477
186.921977	2460.323081	17.704141	-0.036899	2.750323
186.956496	2452.353011	17.709146	-0.036900	2.746232
186.914115	2444.407527	17.714151	-0.036888	2.742144
186.968523	2436.432166	17.719155	-0.036893	2.738039
186.883233	2428.481673	17.724160	-0.036872	2.733933
186.629326	2420.491341	17.729165	-0.036819	2.729790
186.762183	2412.531770	17.734170	-0.036839	2.725680
186.971000	2404.542560	17.739175	-0.036873	2.721554
186.679867	2396.596786	17.744179	-0.036814	2.717412
186.729039	2388.631593	17.749184	-0.036818	2.713276
186.581794	2380.634921	17.754189	-0.036785	2.709104
186.542858	2372.652015	17.759194	-0.036773	2.704940
186.432275	2364.704966	17.764199	-0.036748	2.700784
186.469352	2356.726192	17.769203	-0.036749	2.696614
186.546670	2348.732250	17.774208	-0.036759	2.692432
186.480921	2340.756656	17.779213	-0.036742	2.688244
186.476205	2332.790895	17.784218	-0.036736	2.684058
186.257446	2324.867042	17.789223	-0.036690	2.679875
186.115028	2316.906173	17.794227	-0.036658	2.675670
186.253462	2308.868808	17.799232	-0.036679	2.671436
186.296392	2300.879327	17.804237	-0.036682	2.667215
186.151033	2292.913047	17.809242	-0.036650	2.662987
186.143152	2284.964475	17.814247	-0.036643	2.658771
186.140929	2276.979081	17.819251	-0.036638	2.654529
186.129114	2269.017006	17.824256	-0.036631	2.650292
185.830185	2261.071571	17.829261	-0.036570	2.646038
185.911792	2253.083564	17.834266	-0.036580	2.641779
185.880409	2245.128416	17.839271	-0.036569	2.637524
185.821752	2237.139677	17.844275	-0.036553	2.633242
185.814363	2229.151820	17.849280	-0.036547	2.628957
185.837048	2221.157011	17.854285	-0.036546	2.624663
185.670506	2213.235796	17.859290	-0.036510	2.620389
185.558005	2205.286753	17.864295	-0.036484	2.616097
185.386668	2197.309594	17.869299	-0.036447	2.611778
185.682292	2189.313301	17.874304	-0.036497	2.607474
185.395941	2181.348705	17.879309	-0.036439	2.603140
185.284144	2173.418871	17.884314	-0.036413	2.598830
185.368038	2165.428727	17.889319	-0.036424	2.594493
185.156220	2157.269753	17.894323	-0.036379	2.590036
185.123718	2149.349835	17.899328	-0.036368	2.585715
185.126462	2141.393351	17.904333	-0.036364	2.581368
185.072529	2133.454822	17.909338	-0.036349	2.577021
185.004396	2125.509028	17.914343	-0.036331	2.572660
184.982385	2117.507008	17.919347	-0.036322	2.568265
185.096464	2109.560485	17.924352	-0.036338	2.563903
184.814445	2101.649220	17.929357	-0.036280	2.559524
184.780644	2093.699855	17.934362	-0.036269	2.555135
184.974645	2085.673474	17.939367	-0.036300	2.550711
185.023196	2077.691208	17.944371	-0.036304	2.546294
184.714411	2069.784831	17.949376	-0.036242	2.541886
184.782542	2061.799957	17.954381	-0.036249	2.537453
184.592673	2053.859408	17.959386	-0.036209	2.533019
184.648723	2045.867867	17.964391	-0.036214	2.528567
184.629606	2037.892173	17.969395	-0.036206	2.524109
184.700639	2029.961367	17.974400	-0.036214	2.519676
184.349286	2022.023894	17.979405	-0.036144	2.515201
184.405990	2013.994950	17.984410	-0.036149	2.510695
184.459253	2006.013805	17.989415	-0.036154	2.506209
184.247230	1998.074223	17.994419	-0.036110	2.501718
184.323808	1990.123330	17.999424	-0.036119	2.497234
184.367011	1982.127022	18.004429	-0.036122	2.492713
184.359389	1974.175714	18.009434	-0.036115	2.488207
184.093209	1966.237757	18.014439	-0.036061	2.483680
184.060647	1958.275015	18.019443	-0.036050	2.479149
184.356309	1950.297801	18.024448	-0.036100	2.474625
184.086391	1942.345886	18.029453	-0.036045	2.470065
183.960912	1934.377141	18.034458	-0.036016	2.465498
183.990992	1926.421400	18.039463	-0.036017	2.460942
184.116928	1918.451786	18.044467	-0.036035	2.456376
183.928558	1910.502056	18.049472	-0.035995	2.451790
183.827341	1902.536109	18.054477	-0.035971	2.447192
183.898695	1894.577078	18.059482	-0.035979	2.442603
183.757140	1886.642931	18.064487	-0.035948	2.438003
183.583326	1878.651126	18.069491	-0.035911	2.433358
183.676093	1870.622276	18.074496	-0.035923	2.428704
183.582167	1862.661595	18.079501	-0.035900	2.424066
183.509123	1854.741798	18.084506	-0.035882	2.419444
183.434709	1846.790083	18.089511	-0.035863	2.414795
183.371889	1838.804735	18.094515	-0.035846	2.410118
183.385087	1830.851938	18.099520	-0.035844	2.405457
183.418303	1822.879743	18.104525	-0.035845	2.400777
183.603310	1814.945470	18.109530	-0.035874	2.396123
183.291493	1807.014596	18.114535	-0.035811	2.391422
183.064888	1799.057223	18.119539	-0.035764	2.386702
183.381626	1791.065033	18.124544	-0.035818	2.381996
183.216648	1783.131255	18.129549	-0.035782	2.377277
183.239509	1775.172075	18.134554	-0.035781	2.372549
183.150348	1767.205061	18.139559	-0.035760	2.367797
183.147102	1759.245905	18.144563	-0.035754	2.363047
183.013746	1751.338300	18.149568	-0.035724	2.358308
182.888483	1743.367489	18.154573	-0.035696	2.353523
182.763074	1735.374800	18.159578	-0.035668	2.348714
182.758246	1727.426271	18.164583	-0.035662	2.343932
182.470443	1719.509348	18.169587	-0.035603	2.339136
182.612737	1711.536947	18.174592	-0.035625	2.334332
182.504400	1703.561905	18.179597	-0.035599	2.329495
182.517123	1695.606261	18.184602	-0.035597	2.324671
182.377811	1687.697361	18.189607	-0.035566	2.319852
182.441654	1679.720880	18.194611	-0.035573	2.314999
182.238312	1671.782576	18.199616	-0.035530	2.310137
182.171580	1663.810770	18.204621	-0.035512	2.305255
182.345777	1655.854858	18.209626	-0.035540	2.300393
182.361266	1647.913594	18.214631	-0.035538	2.295516
182.200427	1639.938732	18.219635	-0.035503	2.290593
182.254125	1631.990458	18.224640	-0.035508	2.285695
181.948074	1624.077817	18.229645	-0.035446	2.280777
181.927781	1616.135131	18.234650	-0.035437	2.275854
181.874343	1608.111257	18.239655	-0.035422	2.270867
181.882679	1600.125533	18.244659	-0.035418	2.265898
181.875174	1592.204259	18.249664	-0.035412	2.260958
181.876159	1584.260193	18.254669	-0.035407	2.255993
181.820611	1576.315582	18.259674	-0.035392	2.251011
181.890381	1568.348509	18.264679	-0.035400	2.246016
181.624156	1560.438319	18.269683	-0.035345	2.241015
181.570717	1552.515962	18.274688	-0.035330	2.236015
181.721885	1544.522759	18.279693	-0.035353	2.230976
181.276473	1536.632099	18.284698	-0.035266	2.225939
181.395458	1528.661224	18.289703	-0.035283	2.220889
181.370396	1520.722500	18.294707	-0.035273	2.215835
181.612534	1512.741791	18.299712	-0.035313	2.210767
181.345577	1504.816068	18.304717	-0.035258	2.205676
181.361569	1496.881050	18.309722	-0.035256	2.200593
181.156342	1488.983218	18.314727	-0.035213	2.195502
181.094980	1480.992888	18.319731	-0.035197	2.190353
181.157488	1473.031126	18.324736	-0.035203	2.185222
181.252544	1465.063135	18.329741	-0.035216	2.180077
180.998429	1457.177188	18.334746	-0.035164	2.174942
180.790237	1449.247114	18.339751	-0.035120	2.169769
180.817881	1441.272324	18.344755	-0.035120	2.164577
180.888975	1433.346487	18.349760	-0.035128	2.159409
180.758445	1425.420955	18.354765	-0.035099	2.154209
180.799498	1417.447793	18.359770	-0.035102	2.148982
180.685253	1409.525233	18.364775	-0.035075	2.143760
180.471582	1401.618565	18.369779	-0.035031	2.138527
180.682713	1393.645609	18.374784	-0.035065	2.133278
180.715153	1385.685564	18.379789	-0.035066	2.128007
180.541734	1377.783291	18.384794	-0.035029	2.122742
180.554241	1369.859407	18.389799	-0.035026	2.117467
180.349938	1361.884713	18.394803	-0.034983	2.112124
180.379362	1353.925659	18.399808	-0.034983	2.106800
180.052704	1346.013365	18.404813	-0.034917	2.101460
180.068474	1338.081734	18.409818	-0.034915	2.096127
180.375532	1330.093297	18.414823	-0.034968	2.090770
180.103495	1322.185729	18.419827	-0.034912	2.085397
180.281800	1314.261241	18.424832	-0.034940	2.080043
180.089234	1306.357824	18.429837	-0.034899	2.074653
180.157270	1298.396086	18.434842	-0.034907	2.069235
179.904740	1290.491467	18.439847	-0.034855	2.063810
180.001947	1282.552538	18.444851	-0.034868	2.058382
179.871609	1274.643043	18.449856	-0.034839	2.052937
179.577012	1266.725274	18.454861	-0.034779	2.047455
179.557022	1258.804385	18.459866	-0.034770	2.041985
179.723693	1250.865778	18.464871	-0.034796	2.036506
179.632408	1242.902826	18.469875	-0.034774	2.030969
179.388412	1235.003861	18.474880	-0.034724	2.025446
179.282603	1227.070023	18.479885	-0.034699	2.019897
179.557989	1219.118615	18.484890	-0.034745	2.014361
179.224751	1211.222723	18.489895	-0.034678	2.008785
179.298681	1203.268487	18.494899	-0.034687	2.003195
179.356158	1195.359572	18.499904	-0.034693	1.997619
179.265644	1187.438271	18.504909	-0.034671	1.992003
179.173431	1179.512370	18.509914	-0.034649	1.986368
179.225332	1171.594543	18.514919	-0.034653	1.980739
178.971171	1163.706815	18.519923	-0.034601	1.975082
178.927691	1155.779690	18.524928	-0.034588	1.969402
178.624457	1147.881716	18.529933	-0.034527	1.963700
178.779098	1139.955439	18.534938	-0.034550	1.958010
178.655440	1132.020166	18.539943	-0.034522	1.952266
178.610600	1124.051071	18.544947	-0.034509	1.946490
178.853061	1116.116738	18.549952	-0.034549	1.940753
178.585735	1108.236365	18.554957	-0.034494	1.934983
178.335887	1100.343994	18.559962	-0.034443	1.929188
178.316142	1092.416971	18.564967	-0.034434	1.923376
178.471549	1084.481705	18.569971	-0.034458	1.917560
178.524600	1076.564698	18.574976	-0.034463	1.911728
178.471529	1068.645700	18.579981	-0.034448	1.905865
178.371322	1060.761801	18.584986	-0.034425	1.900004
178.412998	1052.857486	18.589991	-0.034427	1.894127
178.264274	1044.935602	18.594995	-0.034395	1.888196
178.338954	1037.032994	18.600000	-0.034404	1.882286
178.285263	1029.141269	18.605005	-0.034389	1.876351
177.886026	1021.265425	18.610010	-0.034309	1.870370
178.042517	1013.315943	18.615015	-0.034333	1.864378
177.937871	1005.420496	18.620019	-0.034309	1.858377
177.950709	997.518270	18.625024	-0.034306	1.852365
177.792181	989.612815	18.630029	-0.034272	1.846311
177.834459	981.712521	18.635034	-0.034275	1.840265
177.776616	973.835662	18.640039	-0.034259	1.834205
177.705420	965.904032	18.645043	-0.034241	1.828081
177.521898	958.043913	18.650048	-0.034202	1.821978
177.434835	950.150996	18.655053	-0.034181	1.815841
177.384717	942.241474	18.660058	-0.034166	1.809675
177.282736	934.366738	18.665063	-0.034142	1.803508
177.250665	926.476956	18.670067	-0.034131	1.797317
177.260037	918.543163	18.675072	-0.034128	1.791075
177.148112	910.620291	18.680077	-0.034102	1.784805
177.279544	902.727004	18.685082	-0.034122	1.778566
176.909972	894.893775	18.690087	-0.034048	1.772291
176.670164	887.003345	18.695091	-0.033998	1.765964
176.871830	879.096211	18.700096	-0.034031	1.759656
176.777982	871.222075	18.705101	-0.034008	1.753315
176.814116	863.310357	18.710106	-0.034010	1.746936
176.804740	855.444776	18.715111	-0.034004	1.740566
176.651588	847.571824	18.720115	-0.033970	1.734149
176.604685	839.701879	18.725120	-0.033956	1.727723
176.629992	831.811222	18.730125	-0.033956	1.721266
176.767270	823.920532	18.735130	-0.033977	1.714799
176.452449	816.069464	18.740135	-0.033913	1.708281
176.395081	808.180718	18.745139	-0.033897	1.701741
176.609446	800.282938	18.750144	-0.033932	1.695204
176.444709	792.418739	18.755149	-0.033897	1.688619
176.432775	784.554246	18.760154	-0.033890	1.682029
176.290245	776.722707	18.765159	-0.033858	1.675423
176.213136	768.841465	18.770163	-0.033839	1.668757
176.013344	761.011406	18.775168	-0.033797	1.662092
175.911207	753.147582	18.780173	-0.033773	1.655384
176.080750	745.234125	18.785178	-0.033799	1.648643
175.936904	737.404037	18.790183	-0.033768	1.641904
175.718633	729.572871	18.795187	-0.033722	1.635126
175.751774	721.640906	18.800192	-0.033723	1.628266
175.856172	713.758281	18.805197	-0.033738	1.621431
175.813084	705.921103	18.810202	-0.033725	1.614585
175.903921	698.046776	18.815207	-0.033737	1.607697
175.727625	690.214067	18.820211	-0.033699	1.600778
175.830014	682.381452	18.825216	-0.033713	1.593869
175.479345	674.562747	18.830221	-0.033643	1.586877
175.366956	666.738830	18.835226	-0.033617	1.579884
175.394998	658.886252	18.840231	-0.033617	1.572854
175.244305	651.044060	18.845235	-0.033584	1.565776
175.406150	643.196684	18.850240	-0.033609	1.558707
175.234485	635.361982	18.855245	-0.033572	1.551568
175.135646	627.514079	18.860250	-0.033549	1.544395
175.109074	619.707248	18.865255	-0.033539	1.537236
174.793309	611.894073	18.870259	-0.033476	1.529995
174.874606	604.058276	18.875264	-0.033486	1.522759
174.689240	596.257074	18.880269	-0.033446	1.515479
174.728316	588.410696	18.885274	-0.033449	1.508156
174.711231	580.584412	18.890279	-0.033440	1.500808
174.665952	572.766981	18.895283	-0.033427	1.493428
174.667318	564.938792	18.900288	-0.033422	1.486008
174.696849	557.139756	18.905293	-0.033423	1.478583
174.498971	549.320621	18.910298	-0.033381	1.471066
174.430162	541.500660	18.915303	-0.033364	1.463529
174.456810	533.687078	18.920307	-0.033364	1.455975
174.423823	525.886896	18.925312	-0.033353	1.448385
174.311833	518.109652	18.930317	-0.033327	1.440765
174.168098	510.337945	18.935322	-0.033295	1.433104
174.199182	502.529514	18.940327	-0.033296	1.425395
174.069847	494.760389	18.945331	-0.033267	1.417656
174.039083	486.968947	18.950336	-0.033256	1.409868
173.931512	479.197862	18.955341	-0.033231	1.402045
173.892377	471.425368	18.960346	-0.033219	1.394189
173.821782	463.628894	18.965351	-0.033201	1.386257
173.724449	455.870780	18.970355	-0.033178	1.378315
173.762081	448.092652	18.975360	-0.033180	1.370330
173.589200	440.347170	18.980365	-0.033143	1.362295
173.567159	432.593574	18.985370	-0.033134	1.354230
173.592357	424.819985	18.990375	-0.033134	1.346104
173.273953	417.113261	18.995379	-0.033070	1.337939
173.487326	409.319299	19.000384	-0.033105	1.329725
173.430254	401.581624	19.005389	-0.033089	1.321472
173.174489	393.845274	19.010394	-0.033037	1.313132
173.084288	386.025402	19.015399	-0.033015	1.304679
173.107123	378.283448	19.020403	-0.033014	1.296277
173.113924	370.560095	19.025408	-0.033011	1.287837
172.910841	362.876882	19.030413	-0.032968	1.279346
172.739561	355.186759	19.035418	-0.032931	1.270797
172.773770	347.469807	19.040423	-0.032933	1.262199
172.548067	339.793374	19.045427	-0.032886	1.253538
172.677225	332.063372	19.050432	-0.032905	1.244824
172.662570	324.381411	19.055437	-0.032898	1.236076
172.286269	316.722825	19.060442	-0.032823	1.227221
172.214209	309.049384	19.065447	-0.032805	1.218345
172.115711	301.369557	19.070451	-0.032781	1.209391
172.359884	293.660764	19.075456	-0.032822	1.200405
172.112879	286.033891	19.080461	-0.032771	1.191348
171.849191	278.409168	19.085466	-0.032717	1.182222
171.983837	270.731824	19.090471	-0.032737	1.173043
171.878787	263.093967	19.095475	-0.032713	1.163789
171.880496	255.455642	19.100480	-0.032709	1.154484
171.682467	247.806791	19.105485	-0.032667	1.145047
171.770943	240.169311	19.110490	-0.032679	1.135607
171.610157	232.572160	19.115495	-0.032644	1.126085
171.592085	224.971868	19.120499	-0.032636	1.116509
171.628549	217.359181	19.125504	-0.032638	1.106846
171.410438	209.811455	19.130509	-0.032592	1.097125
171.129539	202.261330	19.135514	-0.032535	1.087300
171.414248	194.651630	19.140519	-0.032584	1.077435
170.996469	187.133227	19.145523	-0.032501	1.067439
170.829137	179.609988	19.150528	-0.032465	1.057400
170.832609	172.048390	19.155533	-0.032461	1.047253
170.821619	164.516765	19.160538	-0.032454	1.037044
170.636947	157.022408	19.165543	-0.032415	1.026743
170.588495	149.512759	19.170547	-0.032401	1.016349
170.745445	141.989941	19.175552	-0.032426	1.005879
170.647592	134.522636	19.180557	-0.032403	0.995316
170.607024	127.017154	19.185562	-0.032391	0.984598
170.288408	119.614069	19.190567	-0.032327	0.973841
170.261774	112.158411	19.195571	-0.032317	0.962960
170.265459	104.737937	19.200576	-0.032313	0.952016
170.075644	97.346943	19.205581	-0.032273	0.940938
169.907928	89.970919	19.210586	-0.032237	0.929756
169.833483	82.608462	19.215591	-0.032219	0.918484
169.598299	75.256979	19.220595	-0.032170	0.907045
169.674186	67.900094	19.225600	-0.032180	0.895538
169.547943	60.808363	19.230605	-0.032152	0.884247