Thu Mar 11 18:17:34 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.375994	-0.100722	0.000000	0.000003	0.723961

0.341190	-0.098420	0.005005	0.000010	0.723954
0.242867	-0.081502	0.010010	0.000028	0.723953
0.363310	-0.099589	0.015014	0.000005	0.723960
0.567876	-0.141776	0.020019	-0.000033	0.723949
0.506188	-0.126042	0.025024	-0.000022	0.723958
0.438588	-0.117503	0.030029	-0.000009	0.723952
0.575194	-0.140778	0.035034	-0.000035	0.723954
0.615831	-0.146728	0.040038	-0.000043	0.723957
0.465443	-0.124604	0.045043	-0.000015	0.723949
0.418391	-0.110838	0.050048	-0.000007	0.723959
0.241966	-0.084438	0.055053	0.000026	0.723950
0.221138	-0.080042	0.060058	0.000030	0.723952
0.122089	-0.057896	0.065062	0.000048	0.723961
0.293362	-0.093279	0.070067	0.000016	0.723952
0.241784	-0.102971	0.075072	0.000025	0.723915
-0.035809	-0.199243	0.080077	0.000077	0.723630
0.077783	-0.219696	0.085082	0.000056	0.723630
0.195754	-0.237982	0.090086	0.000033	0.723636
-0.020121	-0.203480	0.095091	0.000073	0.723628
0.074313	-0.217296	0.100096	0.000056	0.723635
0.146046	-0.233244	0.105101	0.000042	0.723629
0.365438	-0.271140	0.110106	0.000001	0.723631
0.381082	-0.416658	0.115110	-0.000002	0.723352
0.357210	-0.423863	0.120115	0.000002	0.723330
0.476136	-0.437901	0.125120	-0.000020	0.723344
0.272402	-0.406673	0.130125	0.000018	0.723335
0.385176	-0.443262	0.135130	-0.000003	0.723303
0.377692	-0.592198	0.140134	-0.000002	0.723008
0.138395	-0.555589	0.145139	0.000042	0.722997
0.213271	-0.564654	0.150144	0.000028	0.723006
0.177085	-0.560509	0.155149	0.000035	0.723002
0.104447	-0.677774	0.160154	0.000048	0.722746
0.342148	-0.747333	0.165158	0.000004	0.722693
0.181263	-0.721103	0.170163	0.000033	0.722689
0.405402	-0.770786	0.175168	-0.000009	0.722670
0.306742	-0.906695	0.180173	0.000010	0.722369
0.231096	-0.892580	0.185178	0.000024	0.722371
0.456926	-0.931430	0.190182	-0.000019	0.722374
0.320569	-1.027658	0.195187	0.000007	0.722138
0.084408	-1.016119	0.200192	0.000050	0.722078
0.209769	-1.042286	0.205197	0.000027	0.722071
0.216055	-1.153414	0.210202	0.000026	0.721855
0.113650	-1.191458	0.215206	0.000044	0.721745
-0.082180	-1.161583	0.220211	0.000081	0.721736
0.091846	-1.292324	0.225216	0.000048	0.721540
0.088649	-1.346461	0.230221	0.000049	0.721433
0.072313	-1.342788	0.235226	0.000051	0.721435
0.295140	-1.523814	0.240230	0.000010	0.721157
0.274469	-1.542745	0.245235	0.000013	0.721113
0.254245	-1.576993	0.250240	0.000017	0.721039
0.156443	-1.639954	0.255245	0.000035	0.720881
0.039014	-1.620144	0.260250	0.000057	0.720879
-0.074693	-1.751563	0.265254	0.000078	0.720581
-0.107261	-1.768675	0.270259	0.000084	0.720537
-0.053514	-1.850796	0.275264	0.000074	0.720394
-0.134157	-1.922844	0.280269	0.000088	0.720224
-0.388077	-1.896997	0.285274	0.000136	0.720187
-0.258587	-2.062426	0.290278	0.000111	0.719907
-0.391627	-2.043716	0.295283	0.000136	0.719897
-0.565300	-2.129791	0.300288	0.000168	0.719667
-1.040194	-2.078673	0.305293	0.000256	0.719601
-1.364178	-2.084796	0.310298	0.000316	0.719476
-2.205219	-2.037536	0.315302	0.000473	0.719274
-2.248901	-2.033350	0.320307	0.000481	0.719268
-2.837348	-2.016163	0.325312	0.000590	0.719095
-3.724551	-1.926715	0.330317	0.000755	0.718960
-3.450761	-1.976972	0.335322	0.000704	0.718958
-3.599392	-1.981588	0.340326	0.000731	0.718897
-4.645956	-1.924995	0.345331	0.000926	0.718641
-4.255886	-1.989833	0.350336	0.000853	0.718651
-4.492210	-1.953073	0.355341	0.000897	0.718640
-4.718891	-1.970066	0.360346	0.000939	0.718527
-4.932963	-2.017680	0.365350	0.000979	0.718359
-5.234849	-1.968449	0.370355	0.001035	0.718350
-5.651634	-1.890532	0.375360	0.001112	0.718358
-5.502761	-1.955656	0.380365	0.001084	0.718282
-6.251129	-1.957226	0.385370	0.001223	0.718016
-6.480129	-1.912321	0.390374	0.001266	0.718024
-6.790279	-1.861852	0.395379	0.001323	0.718015
-6.162985	-1.970175	0.400384	0.001206	0.718022
-6.229833	-2.023129	0.405389	0.001219	0.717895
-7.955634	-1.812299	0.410394	0.001540	0.717704
-7.370945	-1.913826	0.415398	0.001431	0.717710
-7.651686	-1.868395	0.420403	0.001483	0.717701
-7.736288	-1.849842	0.425408	0.001498	0.717708
-7.449913	-1.901987	0.430413	0.001445	0.717706
-7.705915	-1.962516	0.435418	0.001492	0.717497
-8.712252	-1.842118	0.440422	0.001679	0.717381
-8.858289	-1.820677	0.445427	0.001706	0.717372
-8.540773	-1.872014	0.450432	0.001647	0.717383
-8.412863	-1.899447	0.455437	0.001623	0.717374
-8.689809	-1.850188	0.460442	0.001674	0.717374
-8.489244	-1.918073	0.465446	0.001637	0.717311
-9.327390	-1.888616	0.470451	0.001793	0.717075
-9.161842	-1.914585	0.475456	0.001762	0.717082
-9.468744	-1.862001	0.480461	0.001819	0.717078
-9.310192	-1.891064	0.485466	0.001789	0.717077
-9.011863	-1.939737	0.490470	0.001733	0.717086
-9.494689	-1.865168	0.495475	0.001823	0.717064
-9.996915	-1.930798	0.500480	0.001916	0.716757
-10.190684	-1.901204	0.505485	0.001952	0.716748
-10.952924	-1.764118	0.510490	0.002094	0.716751
-10.294429	-1.878606	0.515494	0.001971	0.716757
-10.220653	-1.896315	0.520499	0.001957	0.716748
-10.600614	-1.825510	0.525504	0.002028	0.716755
-10.614044	-1.825673	0.530509	0.002030	0.716750
-11.044023	-1.904098	0.535514	0.002110	0.716444
-11.191426	-1.875074	0.540518	0.002137	0.716449
-11.614364	-1.806468	0.545523	0.002216	0.716437
-11.237121	-1.870309	0.550528	0.002145	0.716444
-11.156120	-1.884454	0.555533	0.002130	0.716444
-11.479582	-1.829429	0.560538	0.002190	0.716440
-11.305543	-1.856914	0.565542	0.002157	0.716447
-11.707964	-1.930526	0.570547	0.002232	0.716160
-12.196345	-1.858532	0.575552	0.002323	0.716130
-12.420710	-1.819660	0.580557	0.002364	0.716129
-12.061895	-1.885461	0.585562	0.002297	0.716125
-12.034465	-1.885730	0.590566	0.002292	0.716135
-12.420631	-1.821897	0.595571	0.002364	0.716125
-12.199669	-1.858216	0.600576	0.002322	0.716132
-12.330254	-1.942925	0.605581	0.002347	0.715918
-13.208930	-1.807621	0.610586	0.002510	0.715876
-13.046346	-1.833306	0.615590	0.002479	0.715883
-12.649718	-1.907104	0.620595	0.002405	0.715877
-12.900030	-1.860419	0.625600	0.002452	0.715882
-12.881419	-1.864593	0.630605	0.002448	0.715881
-12.853642	-1.919274	0.635610	0.002443	0.715782
-13.634807	-1.898267	0.640614	0.002588	0.715549
-13.944608	-1.847559	0.645619	0.002645	0.715540
-14.106187	-1.815657	0.650624	0.002675	0.715547
-13.663241	-1.895856	0.655629	0.002593	0.715545
-14.084369	-1.822441	0.660634	0.002671	0.715542
-14.190364	-1.799339	0.665638	0.002690	0.715550
-14.150846	-1.825267	0.670643	0.002683	0.715513
-14.466692	-1.909219	0.675648	0.002742	0.715236
-14.826075	-1.848533	0.680653	0.002808	0.715229
-15.177644	-1.787822	0.685658	0.002873	0.715226
-14.591485	-1.889483	0.690662	0.002764	0.715232
-14.952528	-1.829603	0.695667	0.002831	0.715223
-15.050164	-1.808267	0.700672	0.002849	0.715232
-14.676605	-1.874887	0.705677	0.002779	0.715232
-15.604055	-1.866893	0.710682	0.002952	0.714920
-15.786949	-1.839219	0.715686	0.002986	0.714911
-15.690656	-1.861282	0.720691	0.002968	0.714902
-15.537479	-1.886637	0.725696	0.002939	0.714906
-16.239094	-1.761360	0.730701	0.003069	0.714907
-16.023732	-1.799523	0.735706	0.003029	0.714907
-15.414766	-1.904504	0.740710	0.002915	0.714915
-16.168799	-1.855223	0.745715	0.003056	0.714746
-17.134216	-1.753126	0.750720	0.003235	0.714608
-16.311830	-1.901479	0.755725	0.003082	0.714605
-16.624124	-1.848468	0.760730	0.003140	0.714600
-16.779147	-1.814946	0.765734	0.003168	0.714612
-16.544928	-1.862720	0.770739	0.003125	0.714600
-16.605926	-1.847521	0.775744	0.003136	0.714609
-16.919037	-1.849240	0.780749	0.003194	0.714496
-17.818978	-1.801296	0.785754	0.003361	0.714273
-17.212476	-1.905649	0.790758	0.003248	0.714280
-17.954760	-1.776973	0.795763	0.003386	0.714274
-17.895514	-1.785321	0.800768	0.003375	0.714278
-17.271945	-1.897783	0.805773	0.003259	0.714276
-17.804557	-1.804576	0.810778	0.003358	0.714273
-17.566979	-1.842809	0.815782	0.003313	0.714282
-18.060741	-1.909888	0.820787	0.003405	0.713974
-18.389976	-1.852833	0.825792	0.003466	0.713971
-18.530894	-1.827956	0.830797	0.003492	0.713971
-18.743389	-1.793507	0.835802	0.003531	0.713965
-18.611603	-1.814033	0.840806	0.003507	0.713971
-18.734850	-1.796585	0.845811	0.003529	0.713962
-18.795475	-1.783224	0.850816	0.003541	0.713968
-18.750189	-1.860794	0.855821	0.003532	0.713830
-19.774649	-1.771274	0.860826	0.003722	0.713646
-19.638595	-1.791032	0.865830	0.003697	0.713655
-19.837432	-1.761055	0.870835	0.003734	0.713644
-19.637908	-1.793339	0.875840	0.003696	0.713651
-19.301657	-1.852338	0.880845	0.003634	0.713653
-19.803829	-1.767689	0.885850	0.003727	0.713644
-19.422544	-1.830000	0.890854	0.003656	0.713656
-19.714856	-1.905003	0.895859	0.003710	0.713403
-20.551199	-1.777881	0.900864	0.003865	0.713360
-20.228643	-1.836835	0.905869	0.003805	0.713358
-20.157643	-1.850930	0.910874	0.003792	0.713355
-20.576735	-1.772526	0.915878	0.003870	0.713363
-20.496534	-1.790301	0.920883	0.003855	0.713356
-20.158646	-1.847945	0.925888	0.003791	0.713362
-20.646921	-1.904334	0.930893	0.003882	0.713077
-21.739506	-1.738210	0.935898	0.004085	0.713021
-21.319476	-1.809276	0.940902	0.004007	0.713028
-21.263026	-1.825210	0.945907	0.003996	0.713017
-21.475956	-1.783617	0.950912	0.004036	0.713025
-21.203255	-1.834042	0.955917	0.003985	0.713022
-21.206681	-1.836327	0.960922	0.003985	0.713016
-21.580858	-1.848043	0.965926	0.004055	0.712861
-22.675886	-1.731378	0.970931	0.004258	0.712705
-22.139556	-1.824464	0.975936	0.004158	0.712710
-22.181647	-1.817507	0.980941	0.004166	0.712709
-22.805488	-1.708462	0.985946	0.004282	0.712706
-22.084316	-1.834248	0.990950	0.004147	0.712711
-22.363937	-1.787084	0.995955	0.004199	0.712706
-22.492821	-1.761722	1.000960	0.004223	0.712712
-22.614173	-1.864576	1.005965	0.004246	0.712464
-23.443411	-1.756705	1.010970	0.004400	0.712385
-23.309516	-1.778127	1.015974	0.004375	0.712390
-23.447125	-1.756383	1.020979	0.004400	0.712385
-23.449153	-1.754643	1.025984	0.004400	0.712388
-23.290351	-1.782345	1.030989	0.004370	0.712390
-23.641616	-1.724098	1.035994	0.004436	0.712381
-23.228004	-1.795439	1.040998	0.004358	0.712387
-23.541273	-1.892277	1.046003	0.004417	0.712083
-23.929322	-1.818191	1.051008	0.004489	0.712093
-24.320331	-1.748433	1.056013	0.004561	0.712094
-24.215359	-1.769912	1.061018	0.004541	0.712088
-24.094383	-1.789660	1.066022	0.004519	0.712092
-24.469451	-1.727287	1.071027	0.004588	0.712084
-24.173686	-1.776887	1.076032	0.004533	0.712090
-24.421864	-1.867560	1.081037	0.004579	0.711822
-25.515981	-1.705321	1.086042	0.004783	0.711757
-25.098552	-1.774334	1.091046	0.004705	0.711768
-25.021201	-1.795274	1.096051	0.004690	0.711754
-25.393434	-1.725534	1.101056	0.004759	0.711761
-25.130184	-1.769617	1.106061	0.004710	0.711767
-25.107982	-1.778852	1.111066	0.004706	0.711757
-25.273328	-1.786179	1.116070	0.004736	0.711684
-26.487175	-1.688377	1.121075	0.004962	0.711448
-25.978564	-1.776615	1.126080	0.004867	0.711454
-25.961095	-1.780034	1.131085	0.004864	0.711453
-26.156028	-1.747288	1.136090	0.004900	0.711450
-26.075271	-1.758228	1.141094	0.004885	0.711457
-26.164072	-1.746702	1.146099	0.004901	0.711449
-25.963622	-1.781593	1.151104	0.004863	0.711451
-26.254420	-1.830707	1.156109	0.004917	0.711250
-27.221976	-1.716370	1.161114	0.005097	0.711134
-26.826725	-1.782142	1.166118	0.005024	0.711144
-26.996077	-1.755556	1.171123	0.005055	0.711137
-27.008428	-1.751550	1.176128	0.005057	0.711141
-26.910820	-1.769602	1.181133	0.005039	0.711140
-26.997676	-1.758068	1.186138	0.005055	0.711133
-26.964174	-1.815616	1.191142	0.005048	0.711030
-27.445293	-1.812298	1.196147	0.005138	0.710866
-27.543732	-1.793303	1.201152	0.005156	0.710869
-27.600980	-1.782978	1.206157	0.005166	0.710870
-27.699077	-1.768306	1.211162	0.005184	0.710865
-27.453075	-1.806742	1.216166	0.005138	0.710876
-28.081361	-1.699270	1.221171	0.005255	0.710867
-28.241256	-1.804373	1.226176	0.005285	0.710601
-28.541199	-1.785617	1.231181	0.005340	0.710532
-29.031524	-1.700616	1.236186	0.005431	0.710528
-28.544560	-1.784029	1.241190	0.005340	0.710535
-28.523927	-1.791530	1.246195	0.005336	0.710527
-28.686533	-1.760045	1.251200	0.005366	0.710533
-28.841634	-1.733063	1.256205	0.005395	0.710532
-29.048937	-1.771406	1.261210	0.005434	0.710382
-29.604345	-1.753790	1.266214	0.005537	0.710220
-29.630032	-1.753386	1.271219	0.005541	0.710212
-29.795538	-1.720487	1.276224	0.005572	0.710219
-29.391869	-1.793317	1.281229	0.005497	0.710218
-29.755245	-1.732264	1.286234	0.005564	0.710210
-29.828462	-1.714172	1.291238	0.005577	0.710221
-29.675737	-1.761029	1.296243	0.005549	0.710182
-30.373367	-1.782345	1.301248	0.005679	0.709891
-30.327210	-1.789042	1.306253	0.005670	0.709895
-30.748631	-1.717915	1.311258	0.005748	0.709887
-30.190914	-1.811915	1.316262	0.005644	0.709898
-30.460121	-1.769437	1.321267	0.005694	0.709888
-30.597440	-1.741524	1.326272	0.005719	0.709895
-29.984582	-1.877518	1.331277	0.005605	0.709842
-31.490244	-1.733489	1.336282	0.005885	0.709594
-31.586062	-1.712933	1.341286	0.005903	0.709601
-31.493966	-1.733516	1.346291	0.005885	0.709593
-31.250187	-1.776917	1.351296	0.005840	0.709593
-31.513819	-1.728327	1.356301	0.005889	0.709597
-31.642396	-1.708334	1.361306	0.005912	0.709592
-31.190494	-1.784455	1.366310	0.005828	0.709601
-31.727398	-1.826447	1.371315	0.005928	0.709326
-32.620313	-1.696675	1.376320	0.006094	0.709267
-32.137821	-1.782114	1.381325	0.006004	0.709269
-32.153841	-1.784597	1.386330	0.006007	0.709259
-32.456242	-1.725821	1.391334	0.006063	0.709269
-32.090780	-1.793952	1.396339	0.005995	0.709263
-32.130089	-1.784522	1.401344	0.006002	0.709268
-32.692857	-1.805030	1.406349	0.006106	0.709027
-33.666189	-1.669097	1.411354	0.006287	0.708952
-32.913907	-1.798723	1.416358	0.006147	0.708961
-33.011656	-1.784025	1.421363	0.006165	0.708956
-33.615402	-1.674350	1.426368	0.006277	0.708961
-33.095087	-1.768209	1.431373	0.006180	0.708959
-33.249364	-1.744450	1.436378	0.006209	0.708952
-33.469092	-1.775839	1.441382	0.006249	0.708811
-34.168680	-1.738522	1.446387	0.006379	0.708636
-33.791671	-1.803061	1.451392	0.006309	0.708642
-34.048342	-1.755867	1.456397	0.006357	0.708645
-34.398507	-1.697037	1.461402	0.006422	0.708639
-33.558909	-1.846244	1.466406	0.006265	0.708640
-33.920596	-1.783957	1.471411	0.006332	0.708636
-34.656439	-1.729013	1.476416	0.006469	0.708484
-34.960022	-1.741278	1.481421	0.006525	0.708351
-34.764719	-1.781262	1.486426	0.006489	0.708341
-35.036568	-1.728520	1.491430	0.006539	0.708350
-35.164431	-1.707906	1.496435	0.006563	0.708346
-34.966477	-1.741547	1.501440	0.006526	0.708350
-34.725267	-1.782819	1.506445	0.006481	0.708354
-35.284631	-1.726037	1.511450	0.006585	0.708268
-35.799583	-1.760721	1.516454	0.006680	0.708015
-35.697709	-1.781132	1.521459	0.006661	0.708011
-36.330115	-1.668797	1.526464	0.006779	0.708010
-35.890560	-1.744918	1.531469	0.006697	0.708015
-35.773400	-1.770661	1.536474	0.006675	0.708006
-36.033614	-1.720733	1.541478	0.006723	0.708013
-36.146117	-1.704958	1.546483	0.006744	0.708005
-36.334463	-1.798156	1.551488	0.006779	0.707751
-36.724604	-1.752933	1.556493	0.006851	0.707703
-37.300649	-1.655156	1.561498	0.006958	0.707693
-36.724395	-1.754166	1.566502	0.006851	0.707701
-36.921252	-1.723042	1.571507	0.006887	0.707694
-37.312581	-1.654609	1.576512	0.006960	0.707691
-36.939777	-1.717317	1.581517	0.006890	0.707699
-36.896513	-1.768370	1.586522	0.006882	0.707613
-37.874047	-1.710985	1.591526	0.007064	0.707379
-37.508223	-1.779647	1.596531	0.006995	0.707372
-37.629105	-1.758446	1.601536	0.007018	0.707372
-37.720527	-1.740395	1.606541	0.007034	0.707376
-37.982348	-1.696172	1.611546	0.007083	0.707371
-37.831878	-1.719759	1.616550	0.007055	0.707378
-37.677902	-1.767424	1.621555	0.007026	0.707338
-38.720810	-1.710271	1.626560	0.007220	0.707080
-38.454286	-1.756218	1.631565	0.007170	0.707083
-38.528444	-1.747815	1.636570	0.007184	0.707074
-38.467022	-1.754676	1.641574	0.007172	0.707083
-38.728727	-1.709189	1.646579	0.007221	0.707081
-38.527763	-1.745200	1.651584	0.007183	0.707081
-38.101569	-1.862333	1.656589	0.007104	0.706998
-39.786010	-1.686755	1.661594	0.007417	0.706748
-39.210748	-1.786105	1.666598	0.007310	0.706755
-39.342856	-1.765933	1.671603	0.007334	0.706749
-39.538886	-1.728498	1.676608	0.007370	0.706754
-39.485237	-1.737551	1.681613	0.007360	0.706756
-39.357284	-1.765289	1.686618	0.007336	0.706746
-39.139674	-1.865736	1.691622	0.007295	0.706623
-40.534712	-1.709007	1.696627	0.007555	0.706438
-40.306595	-1.747063	1.701632	0.007512	0.706444
-40.342820	-1.740057	1.706637	0.007519	0.706445
-40.433306	-1.729049	1.711642	0.007535	0.706435
-40.045434	-1.792864	1.716646	0.007463	0.706446
-39.904633	-1.821725	1.721651	0.007437	0.706439
-40.466616	-1.816534	1.726656	0.007541	0.706249
-41.459158	-1.698576	1.731661	0.007726	0.706131
-41.045755	-1.775564	1.736666	0.007649	0.706124
-40.923928	-1.794054	1.741670	0.007626	0.706131
-41.338953	-1.723871	1.746675	0.007703	0.706124
-41.144586	-1.758320	1.751680	0.007666	0.706125
-40.634291	-1.848738	1.756685	0.007571	0.706126
-41.525854	-1.797401	1.761690	0.007737	0.705910
-42.222602	-1.695545	1.766694	0.007866	0.705866
-41.940768	-1.749972	1.771699	0.007814	0.705858
-41.841114	-1.766646	1.776704	0.007795	0.705860
-42.172629	-1.706768	1.781709	0.007857	0.705862
-41.954046	-1.748562	1.786714	0.007816	0.705857
-41.766953	-1.778106	1.791718	0.007781	0.705865
-42.435338	-1.813952	1.796723	0.007905	0.705553
-43.032626	-1.722830	1.801728	0.008016	0.705523
-42.648064	-1.791381	1.806733	0.007944	0.705523
-42.793303	-1.771535	1.811738	0.007971	0.705512
-42.996556	-1.728044	1.816742	0.008009	0.705527
-42.765999	-1.772748	1.821747	0.007965	0.705520
-42.938066	-1.742457	1.826752	0.007997	0.705519
-43.338860	-1.821775	1.831757	0.008072	0.705216
-43.774625	-1.750406	1.836762	0.008153	0.705204
-43.782511	-1.745894	1.841766	0.008154	0.705211
-43.824192	-1.739932	1.846771	0.008162	0.705208
-43.914212	-1.724538	1.851776	0.008178	0.705207
-43.472641	-1.802052	1.856781	0.008096	0.705210
-43.711772	-1.770738	1.861786	0.008140	0.705187
-44.589257	-1.764068	1.866790	0.008303	0.704886
-44.631225	-1.759411	1.871795	0.008311	0.704881
-44.666138	-1.751981	1.876800	0.008317	0.704884
-44.571831	-1.767239	1.881805	0.008299	0.704887
-44.682145	-1.752684	1.886810	0.008320	0.704877
-44.453970	-1.789909	1.891814	0.008277	0.704885
-44.491491	-1.794414	1.896819	0.008284	0.704862
-45.452618	-1.762377	1.901824	0.008463	0.704582
-45.473597	-1.754992	1.906829	0.008466	0.704590
-45.618713	-1.733764	1.911834	0.008493	0.704581
-45.536501	-1.743962	1.916838	0.008478	0.704590
-45.426585	-1.765878	1.921843	0.008457	0.704586
-45.366428	-1.779039	1.926848	0.008446	0.704582
-45.544072	-1.745737	1.931853	0.008478	0.704585
-46.436059	-1.752834	1.936858	0.008644	0.704251
-46.304534	-1.773607	1.941862	0.008620	0.704257
-46.545945	-1.731106	1.946867	0.008664	0.704256
-46.641471	-1.715387	1.951872	0.008682	0.704254
-46.363443	-1.759956	1.956877	0.008630	0.704264
-46.367785	-1.765179	1.961882	0.008631	0.704252
-46.624326	-1.715682	1.966886	0.008678	0.704260
-46.665239	-1.800126	1.971891	0.008686	0.704076
-47.663626	-1.685901	1.976896	0.008871	0.703947
-47.165829	-1.771978	1.981901	0.008778	0.703953
-47.544276	-1.709029	1.986906	0.008849	0.703944
-47.450883	-1.720452	1.991910	0.008831	0.703955
-47.276986	-1.754044	1.996915	0.008798	0.703951
-47.454411	-1.725536	2.001920	0.008831	0.703945

-47.935145	-1.795271	2.011917	0.008920	0.703632
-48.314453	-1.726511	2.021914	0.008991	0.703635
-48.268340	-1.735963	2.031910	0.008982	0.703633
-48.016461	-1.780242	2.041907	0.008934	0.703635
-48.164098	-1.754763	2.051904	0.008961	0.703634
-48.309639	-1.730664	2.061901	0.008988	0.703631
-48.062522	-1.775334	2.071898	0.008942	0.703631
-48.237299	-1.743466	2.081894	0.008974	0.703633
-48.223619	-1.746438	2.091891	0.008971	0.703633
-47.978070	-1.718011	2.101888	0.008925	0.703779
-47.289567	-1.757886	2.111885	0.008796	0.703947
-47.418327	-1.734262	2.121882	0.008820	0.703949
-47.497076	-1.719825	2.131878	0.008834	0.703951
-47.324039	-1.750511	2.141875	0.008802	0.703952
-47.519964	-1.715919	2.151872	0.008838	0.703952
-47.268979	-1.734348	2.161869	0.008790	0.704006
-46.688168	-1.713091	2.171866	0.008682	0.704258
-46.377181	-1.769029	2.181862	0.008624	0.704258
-46.328838	-1.778530	2.191859	0.008614	0.704257
-46.469939	-1.752434	2.201856	0.008640	0.704260
-45.932179	-1.744005	2.211853	0.008540	0.704471
-45.881291	-1.694743	2.221850	0.008530	0.704589
-45.638102	-1.737119	2.231846	0.008484	0.704592
-45.420526	-1.776132	2.241843	0.008443	0.704592
-45.205273	-1.723033	2.251840	0.008403	0.704777
-44.603470	-1.775877	2.261837	0.008290	0.704887
-45.020486	-1.704240	2.271834	0.008367	0.704883
-44.702048	-1.761388	2.281830	0.008308	0.704883
-44.150334	-1.722547	2.291827	0.008205	0.705160
-43.825646	-1.756081	2.301824	0.008144	0.705210
-43.823170	-1.758298	2.311821	0.008143	0.705207
-43.871424	-1.730897	2.321818	0.008152	0.705245
-43.052418	-1.742503	2.331814	0.007999	0.705517
-42.793549	-1.787437	2.341811	0.007950	0.705520
-43.131964	-1.727331	2.351808	0.008013	0.705520
-42.615757	-1.734668	2.361805	0.007916	0.705691
-42.083159	-1.748634	2.371802	0.007817	0.705855
-41.933089	-1.775143	2.381798	0.007788	0.705856
-42.144708	-1.736592	2.391795	0.007827	0.705859
-41.554656	-1.738236	2.401792	0.007717	0.706068
-41.542382	-1.714060	2.411789	0.007714	0.706121
-41.510295	-1.721441	2.421786	0.007708	0.706119
-40.849198	-1.754604	2.431782	0.007584	0.706290
-40.551559	-1.732677	2.441779	0.007529	0.706441
-40.633266	-1.719152	2.451776	0.007543	0.706440
-40.510691	-1.713572	2.461773	0.007520	0.706496
-39.763265	-1.722351	2.471770	0.007381	0.706747
-39.672314	-1.739797	2.481766	0.007363	0.706745
-39.849885	-1.708678	2.491763	0.007396	0.706745
-38.871916	-1.734721	2.501760	0.007214	0.707043
-38.720646	-1.746959	2.511757	0.007185	0.707073
-38.995385	-1.699416	2.521754	0.007236	0.707071
-38.593403	-1.706551	2.531750	0.007160	0.707202
-38.008312	-1.726722	2.541747	0.007051	0.707371
-37.700159	-1.781248	2.551744	0.006993	0.707373
-37.961740	-1.736519	2.561741	0.007042	0.707370
-37.099891	-1.733731	2.571738	0.006881	0.707684
-36.873767	-1.769076	2.581734	0.006838	0.707695
-36.998587	-1.747829	2.591731	0.006861	0.707694
-36.854189	-1.720211	2.601728	0.006834	0.707801
-36.120639	-1.749769	2.611725	0.006697	0.708005
-35.981286	-1.773971	2.621722	0.006671	0.708007
-35.905737	-1.788361	2.631718	0.006656	0.708006
-35.546713	-1.736392	2.641715	0.006589	0.708239
-35.214982	-1.742938	2.651712	0.006527	0.708345
-35.107680	-1.762753	2.661709	0.006506	0.708345
-35.069667	-1.749547	2.671706	0.006499	0.708386
-34.528981	-1.720798	2.681702	0.006398	0.708637
-34.517629	-1.723863	2.691699	0.006395	0.708636
-34.286594	-1.765301	2.701696	0.006352	0.708636
-33.861748	-1.712189	2.711693	0.006272	0.708895
-33.448177	-1.758095	2.721690	0.006195	0.708951
-33.302677	-1.782921	2.731686	0.006167	0.708954
-33.470820	-1.707853	2.741683	0.006198	0.709045
-32.469007	-1.777720	2.751680	0.006011	0.709263
-32.784832	-1.722553	2.761677	0.006070	0.709262
-32.777343	-1.723328	2.771674	0.006068	0.709264
-31.993635	-1.713382	2.781670	0.005922	0.709564
-31.781202	-1.736304	2.791667	0.005882	0.709594
-31.643749	-1.760866	2.801664	0.005856	0.709595
-31.732477	-1.678103	2.811661	0.005872	0.709730
-30.829870	-1.758903	2.821658	0.005703	0.709891
-30.953053	-1.737993	2.831654	0.005726	0.709889
-30.990038	-1.723532	2.841651	0.005732	0.709906
-30.154689	-1.718260	2.851648	0.005577	0.710215
-30.198327	-1.710510	2.861645	0.005584	0.710215
-29.986191	-1.750648	2.871642	0.005544	0.710211
-29.506788	-1.734295	2.881638	0.005455	0.710415
-28.925450	-1.780408	2.891635	0.005346	0.710531
-29.105025	-1.748120	2.901632	0.005379	0.710532
-29.206171	-1.731647	2.911629	0.005398	0.710530
-28.399278	-1.713052	2.921626	0.005247	0.710855
-28.342301	-1.717086	2.931622	0.005236	0.710868
-28.332665	-1.718007	2.941619	0.005234	0.710870
-27.912208	-1.714892	2.951616	0.005155	0.711027
-27.674266	-1.702616	2.961613	0.005110	0.711137
-27.530931	-1.729084	2.971610	0.005083	0.711136
-27.530016	-1.688778	2.981606	0.005083	0.711217
-26.436958	-1.766221	2.991603	0.004879	0.711452
-26.501808	-1.754573	3.001600	0.004890	0.711453
-26.774813	-1.707792	3.011597	0.004941	0.711450
-25.816570	-1.755720	3.021594	0.004762	0.711696
-25.973090	-1.698028	3.031590	0.004791	0.711756
-25.502224	-1.780781	3.041587	0.004703	0.711759
-25.689160	-1.698026	3.051584	0.004737	0.711858
-24.816292	-1.739918	3.061581	0.004574	0.712086
-24.757680	-1.751563	3.071578	0.004563	0.712084
-24.919662	-1.721314	3.081574	0.004593	0.712087
-24.017223	-1.769453	3.091571	0.004424	0.712313
-24.047113	-1.729629	3.101568	0.004429	0.712382
-23.901870	-1.757260	3.111565	0.004402	0.712379
-23.900759	-1.723427	3.121562	0.004401	0.712448
-23.144751	-1.730614	3.131558	0.004260	0.712703
-22.866279	-1.779354	3.141555	0.004208	0.712705
-23.261521	-1.709151	3.151552	0.004281	0.712705
-22.556415	-1.713854	3.161549	0.004149	0.712947
-22.341780	-1.719255	3.171546	0.004109	0.713013
-22.154125	-1.752479	3.181542	0.004074	0.713014
-22.088811	-1.700283	3.191539	0.004061	0.713142
-21.250324	-1.745170	3.201536	0.003905	0.713351
-21.133851	-1.765239	3.211533	0.003883	0.713353
-21.215970	-1.752794	3.221530	0.003898	0.713349
-20.974890	-1.694469	3.231526	0.003852	0.713551
-20.387341	-1.751815	3.241523	0.003742	0.713646
-20.626741	-1.710248	3.251520	0.003787	0.713645
-20.187365	-1.746612	3.261517	0.003704	0.713729
-19.434198	-1.764837	3.271514	0.003564	0.713960
-19.284732	-1.790193	3.281510	0.003536	0.713963
-19.414592	-1.765272	3.291507	0.003559	0.713968
-19.199124	-1.709921	3.301504	0.003519	0.714155
-18.360489	-1.800466	3.311501	0.003362	0.714272
-18.677782	-1.744197	3.321498	0.003421	0.714273
-18.386898	-1.795651	3.331494	0.003366	0.714274
-17.674769	-1.765612	3.341491	0.003233	0.714586
-17.726389	-1.747268	3.351488	0.003243	0.714605
-17.243947	-1.834383	3.361485	0.003152	0.714604
-17.547399	-1.761726	3.371482	0.003209	0.714641
-16.704661	-1.780465	3.381478	0.003051	0.714903
-16.606737	-1.796083	3.391475	0.003033	0.714907
-16.719468	-1.777638	3.401472	0.003053	0.714905
-16.192801	-1.793508	3.411469	0.002955	0.715060
-15.714519	-1.795539	3.421466	0.002865	0.715226
-15.746733	-1.790099	3.431462	0.002871	0.715226
-15.746584	-1.789203	3.441459	0.002870	0.715229
-15.033924	-1.797419	3.451456	0.002737	0.715465
-14.791582	-1.801673	3.461453	0.002692	0.715543
-14.871475	-1.788922	3.471450	0.002706	0.715541
-14.584502	-1.837545	3.481446	0.002653	0.715547
-13.950038	-1.781928	3.491443	0.002534	0.715882
-13.660535	-1.834035	3.501440	0.002480	0.715881
-13.716545	-1.825067	3.511437	0.002490	0.715880
-14.075428	-1.728781	3.521434	0.002556	0.715945
-12.834843	-1.858721	3.531430	0.002325	0.716126
-12.995856	-1.828878	3.541427	0.002354	0.716129
-12.858876	-1.852829	3.551424	0.002328	0.716131
-12.442947	-1.818951	3.561421	0.002251	0.716345
-12.103704	-1.830585	3.571418	0.002187	0.716443
-11.969310	-1.853403	3.581414	0.002162	0.716446
-12.172730	-1.804837	3.591411	0.002199	0.716471
-11.367983	-1.806839	3.601408	0.002049	0.716751
-10.947056	-1.882867	3.611405	0.001970	0.716750
-11.151243	-1.846992	3.621402	0.002008	0.716750
-10.932829	-1.814127	3.631398	0.001967	0.716893
-10.167334	-1.855704	3.641395	0.001824	0.717081
-10.191970	-1.850193	3.651392	0.001828	0.717084
-10.293449	-1.833167	3.661389	0.001846	0.717083
-9.618252	-1.840611	3.671386	0.001720	0.717306
-9.231750	-1.874305	3.681382	0.001648	0.717377
-9.332288	-1.855984	3.691379	0.001666	0.717378
-9.212469	-1.861895	3.701376	0.001644	0.717409
-8.747381	-1.799200	3.711373	0.001557	0.717698
-8.452029	-1.850603	3.721370	0.001501	0.717701
-8.412952	-1.857980	3.731366	0.001494	0.717701
-8.064387	-1.824266	3.741363	0.001428	0.717891
-7.416800	-1.875433	3.751360	0.001307	0.718019
-7.767674	-1.815056	3.761357	0.001372	0.718015
-7.442009	-1.865171	3.771354	0.001311	0.718031
-6.686478	-1.836774	3.781350	0.001170	0.718354
-6.366947	-1.893628	3.791347	0.001110	0.718355
-6.179337	-1.928252	3.801344	0.001075	0.718353
-6.649689	-1.823760	3.811341	0.001162	0.718395
-5.615849	-1.885033	3.821338	0.000969	0.718638
-5.477933	-1.910370	3.831334	0.000943	0.718637
-5.665385	-1.875937	3.841331	0.000978	0.718640
-5.324522	-1.864279	3.851328	0.000914	0.718784
-4.900713	-1.852603	3.861325	0.000834	0.718957
-4.669061	-1.893802	3.871322	0.000791	0.718957
-4.602020	-1.906714	3.881318	0.000778	0.718956
-4.093210	-1.872073	3.891315	0.000683	0.719204
-3.776908	-1.897039	3.901312	0.000624	0.719267
-3.882853	-1.878747	3.911309	0.000643	0.719266
-3.806965	-1.861370	3.921306	0.000628	0.719328
-2.919789	-1.883694	3.931302	0.000463	0.719596
-2.922748	-1.882791	3.941299	0.000463	0.719598
-2.765125	-1.910090	3.951296	0.000433	0.719600
-2.688823	-1.844032	3.961293	0.000419	0.719758
-2.403060	-1.826287	3.971290	0.000365	0.719894
-2.292659	-1.845731	3.981286	0.000344	0.719895
-2.174031	-1.808442	3.991283	0.000322	0.720011
-1.769381	-1.775016	4.001280	0.000246	0.720219
-1.882595	-1.752891	4.011277	0.000266	0.720224
-1.639711	-1.729882	4.021274	0.000221	0.720355
-1.373413	-1.685343	4.031270	0.000171	0.720537
-1.429094	-1.674456	4.041267	0.000181	0.720539
-1.430436	-1.537232	4.051264	0.000181	0.720810
-1.216755	-1.541184	4.061261	0.000140	0.720877
-1.031453	-1.512189	4.071258	0.000105	0.721000
-0.761796	-1.500390	4.081254	0.000055	0.721119
-0.880688	-1.421974	4.091251	0.000077	0.721232
-0.743916	-1.342208	4.101248	0.000051	0.721437
-0.750013	-1.277967	4.111245	0.000051	0.721562
-0.650607	-1.205180	4.121242	0.000032	0.721741
-0.616631	-1.104131	4.131238	0.000026	0.721952
-0.604860	-1.044698	4.141235	0.000023	0.722074
-0.497054	-0.916742	4.151232	0.000002	0.722363
-0.553476	-0.829007	4.161229	0.000012	0.722517
-0.355310	-0.777665	4.171226	-0.000025	0.722687
-0.472788	-0.599989	4.181222	-0.000004	0.722996
-0.457170	-0.492334	4.191219	-0.000007	0.723213
-0.332743	-0.400352	4.201216	-0.000031	0.723437
-0.346133	-0.283238	4.211213	-0.000028	0.723663
-0.250859	-0.154120	4.221210	-0.000047	0.723950
-0.174346	-0.025195	4.231206	-0.000061	0.724230
-0.085905	0.099347	4.241203	-0.000078	0.724505
0.000000	0.232392	4.251200	-0.000095	0.724796

0.126577	0.843170	4.256205	-0.000119	0.726035
0.053670	2.118226	4.261210	-0.000106	0.728496
0.302212	3.945588	4.266214	-0.000154	0.732131
0.680561	6.287393	4.271219	-0.000226	0.736783
0.881546	9.184488	4.276224	-0.000266	0.742407
1.006458	12.573523	4.281229	-0.000291	0.748896
1.352050	16.361608	4.286234	-0.000359	0.756150
1.583426	20.592867	4.291238	-0.000405	0.764121
2.029444	25.175880	4.296243	-0.000491	0.772726
2.427023	30.139337	4.301248	-0.000568	0.781910
2.789937	35.458639	4.306253	-0.000639	0.791614
2.725746	41.154266	4.311258	-0.000631	0.801732
3.276415	47.056904	4.316262	-0.000738	0.812276
3.816656	53.234139	4.321267	-0.000843	0.823155
4.291407	59.710289	4.326272	-0.000936	0.834379
4.719832	66.402414	4.331277	-0.001020	0.845803
5.416606	73.274624	4.336282	-0.001154	0.857451
6.088987	80.372830	4.341286	-0.001284	0.869303
6.300735	87.719190	4.346291	-0.001329	0.881265
6.929558	95.177586	4.351296	-0.001451	0.893361
7.698954	102.784364	4.356301	-0.001599	0.905566
8.302037	110.549753	4.361306	-0.001717	0.917807
9.148308	118.400501	4.366310	-0.001880	0.930083
10.149986	126.336126	4.371315	-0.002072	0.942367
10.490175	134.501270	4.376320	-0.002141	0.954661
10.963606	142.715524	4.381325	-0.002234	0.966905
12.775457	150.783283	4.386330	-0.002577	0.979121
13.592638	159.140531	4.391334	-0.002735	0.991352
14.140843	167.572751	4.396339	-0.002843	1.003473
14.725943	176.051500	4.401344	-0.002957	1.015523
15.305372	184.562463	4.406349	-0.003071	1.027474
16.322929	193.038188	4.411354	-0.003266	1.039343
17.227961	201.576546	4.416358	-0.003440	1.051136
17.876319	210.170525	4.421363	-0.003567	1.062812
18.473979	218.816361	4.426368	-0.003684	1.074418
19.184142	227.430095	4.431373	-0.003822	1.085883
19.757137	236.081473	4.436378	-0.003935	1.097246
20.587422	244.699294	4.441382	-0.004095	1.108506
21.001867	253.381521	4.446387	-0.004178	1.119643
21.743356	262.014372	4.451392	-0.004322	1.130679
22.760112	270.599091	4.456397	-0.004517	1.141606
23.367540	279.273149	4.461402	-0.004636	1.152454
23.643246	287.973896	4.466406	-0.004693	1.163162
24.602184	296.518964	4.471411	-0.004878	1.173726
25.245897	305.120981	4.476416	-0.005003	1.184200
25.854454	313.739886	4.481421	-0.005122	1.194593
26.449878	322.318411	4.486426	-0.005239	1.204847
26.963590	330.925448	4.491430	-0.005340	1.215031
27.564982	339.485687	4.496435	-0.005458	1.225093
28.364798	348.041682	4.501440	-0.005613	1.235107
28.767680	356.606184	4.506445	-0.005694	1.244973
28.999825	365.189848	4.511450	-0.005743	1.254750
29.627470	373.684851	4.516454	-0.005865	1.264427
30.468827	382.146367	4.521459	-0.006028	1.274033
30.967255	390.643123	4.526464	-0.006126	1.283541
31.414848	399.160683	4.531469	-0.006215	1.292993
31.836482	407.633370	4.536474	-0.006300	1.302323
32.559434	416.152345	4.541478	-0.006440	1.311691
32.840536	424.665542	4.546483	-0.006498	1.320906
33.280086	433.090429	4.551488	-0.006586	1.329992
33.689604	441.517052	4.556493	-0.006668	1.339012
34.306832	449.884678	4.561498	-0.006788	1.347946
34.909883	458.280473	4.566502	-0.006906	1.356848
35.378275	466.648971	4.571507	-0.006999	1.365640
35.771132	475.046340	4.576512	-0.007078	1.374392
36.160851	483.424868	4.581517	-0.007156	1.383069
36.344791	491.831074	4.586522	-0.007196	1.391685
37.085361	500.140684	4.591526	-0.007339	1.400244
37.355488	508.493928	4.596531	-0.007395	1.408716
37.997324	516.805077	4.601536	-0.007520	1.417156
38.547843	525.112447	4.606541	-0.007629	1.425528
38.906063	533.460807	4.611546	-0.007701	1.433859
39.316175	541.781281	4.616550	-0.007783	1.442123
39.378042	550.143865	4.621555	-0.007800	1.450326
39.949516	558.431778	4.626560	-0.007912	1.458490
40.463005	566.718012	4.631565	-0.008013	1.466599
40.544273	575.107462	4.636570	-0.008034	1.474693
41.059570	583.362809	4.641574	-0.008136	1.482683
41.512766	591.621204	4.646579	-0.008226	1.490624
42.032182	599.870216	4.651584	-0.008328	1.498523
42.644086	608.100930	4.656589	-0.008447	1.506378
42.930826	616.396421	4.661594	-0.008506	1.514203
43.428599	624.633987	4.666598	-0.008605	1.521965
43.572758	632.928478	4.671603	-0.008637	1.529688
44.064907	641.170166	4.676608	-0.008734	1.537375
44.305838	649.435106	4.681613	-0.008785	1.545007
44.765248	657.683642	4.686618	-0.008876	1.552620
45.088147	665.927112	4.691622	-0.008942	1.560170
45.286060	674.181755	4.696627	-0.008984	1.567675
45.842485	682.383850	4.701632	-0.009093	1.575150
46.375432	690.589991	4.706637	-0.009198	1.582589
46.632778	698.828109	4.711642	-0.009251	1.589982
47.072469	707.053780	4.716646	-0.009339	1.597356
47.634022	715.231430	4.721651	-0.009449	1.604671
48.142329	723.440531	4.726656	-0.009549	1.611972
48.586571	731.655097	4.731661	-0.009637	1.619237
49.058664	739.836506	4.736666	-0.009731	1.626443
49.523591	748.115167	4.741670	-0.009823	1.633701
49.762432	756.312855	4.746675	-0.009873	1.640826
50.051234	764.508556	4.751680	-0.009932	1.647924
50.298478	772.731441	4.756685	-0.009984	1.655010
50.567995	780.917834	4.761690	-0.010040	1.662038
50.861448	789.121432	4.766694	-0.010100	1.669053
51.360577	797.286094	4.771699	-0.010198	1.676034
51.991155	805.413724	4.776704	-0.010321	1.682972
52.398029	813.599264	4.781709	-0.010402	1.689900
52.885805	821.766624	4.786714	-0.010499	1.696796
53.322994	829.946263	4.791718	-0.010586	1.703666
53.689649	838.135846	4.796723	-0.010659	1.710508
54.290560	846.305677	4.801728	-0.010777	1.717337
54.767087	854.449753	4.806733	-0.010871	1.724101
55.259861	862.601848	4.811738	-0.010968	1.730848
55.544421	870.812621	4.816742	-0.011027	1.737589
55.600948	879.005761	4.821747	-0.011043	1.744261
56.127105	887.154204	4.826752	-0.011146	1.750930
56.724335	895.299541	4.831757	-0.011263	1.757581
56.776228	903.484239	4.836762	-0.011278	1.764169
57.319864	911.627486	4.841766	-0.011385	1.770761
57.635674	919.804189	4.846771	-0.011449	1.777327
57.793798	927.980528	4.851776	-0.011484	1.783849
58.082647	936.173003	4.856781	-0.011544	1.790376
58.516317	944.343721	4.861786	-0.011630	1.796879
58.874805	952.464088	4.866790	-0.011702	1.803311
59.578049	960.558512	4.871795	-0.011839	1.809741
60.100293	968.685148	4.876800	-0.011941	1.816151
60.484749	976.828319	4.881805	-0.012018	1.822534
60.709179	984.980727	4.886810	-0.012066	1.828884
61.409124	993.091385	4.891814	-0.012202	1.835235
61.502007	1001.260143	4.896819	-0.012224	1.841538
62.076795	1009.355958	4.901824	-0.012337	1.847819
62.683940	1017.488825	4.906829	-0.012455	1.854112
63.150712	1025.607191	4.911834	-0.012548	1.860355
63.508650	1033.764983	4.916838	-0.012620	1.866595
63.770715	1041.945033	4.921843	-0.012674	1.872819
64.306688	1050.060254	4.926848	-0.012780	1.879005
64.566104	1058.185185	4.931853	-0.012833	1.885147
64.861909	1066.317784	4.936858	-0.012894	1.891279
65.364048	1074.451380	4.941862	-0.012993	1.897414
65.778394	1082.552053	4.946867	-0.013076	1.903496
66.192220	1090.685209	4.951872	-0.013158	1.909581
66.286107	1098.868389	4.956877	-0.013181	1.915649
66.941755	1106.910536	4.961882	-0.013309	1.921656
67.040659	1115.084553	4.966886	-0.013333	1.927679
66.921414	1123.281298	4.971891	-0.013316	1.933676
67.181408	1131.390732	4.976896	-0.013370	1.939633
67.605165	1139.478633	4.981901	-0.013454	1.945573
68.035040	1147.599760	4.986906	-0.013540	1.951520
68.406049	1155.728111	4.991910	-0.013614	1.957448
68.765636	1163.798280	4.996915	-0.013687	1.963314
69.266022	1171.880767	5.001920	-0.013785	1.969187
69.377191	1180.057266	5.006925	-0.013812	1.975068
69.528392	1188.147211	5.011930	-0.013845	1.980874
70.015753	1196.234641	5.016934	-0.013941	1.986696
70.329724	1204.354874	5.021939	-0.014005	1.992507
70.601965	1212.460776	5.026944	-0.014062	1.998286
71.127676	1220.539977	5.031949	-0.014165	2.004056
70.961774	1228.704580	5.036954	-0.014140	2.009797
71.292231	1236.820768	5.041958	-0.014207	2.015540
71.759730	1244.883083	5.046963	-0.014299	2.021242
72.021413	1252.992674	5.051968	-0.014353	2.026940
72.339073	1261.135005	5.056973	-0.014418	2.032651
72.506720	1269.234240	5.061978	-0.014455	2.038300
73.160736	1277.274710	5.066982	-0.014582	2.043942
73.228815	1285.399065	5.071987	-0.014600	2.049568
73.565159	1293.504232	5.076992	-0.014668	2.055191
73.806995	1301.602990	5.081997	-0.014719	2.060786
74.039209	1309.683666	5.087002	-0.014767	2.066351
74.365009	1317.794153	5.092006	-0.014834	2.071932
74.693356	1325.892041	5.097011	-0.014900	2.077489
75.253723	1333.923892	5.102016	-0.015010	2.083009
75.631078	1342.028068	5.107021	-0.015086	2.088545
76.050568	1350.129698	5.112026	-0.015169	2.094069
76.511497	1358.218575	5.117030	-0.015261	2.099574
76.859497	1366.301988	5.122035	-0.015331	2.105050
77.037948	1374.450805	5.127040	-0.015370	2.110539
77.375114	1382.592706	5.132045	-0.015438	2.116024
77.579097	1390.656812	5.137050	-0.015481	2.121430
77.648323	1398.769511	5.142054	-0.015500	2.126842
77.961890	1406.853460	5.147059	-0.015563	2.132244
78.393516	1414.910560	5.152064	-0.015649	2.137626
78.721865	1422.987046	5.157069	-0.015716	2.142998
78.851881	1431.089477	5.162074	-0.015746	2.148354
79.197335	1439.191173	5.167078	-0.015815	2.153717
79.531628	1447.255391	5.172083	-0.015883	2.159040
79.798977	1455.314470	5.177088	-0.015938	2.164341
80.173831	1463.399511	5.182093	-0.016014	2.169656
80.523644	1471.487119	5.187098	-0.016084	2.174957
80.656248	1479.594801	5.192102	-0.016114	2.180238
81.063738	1487.646379	5.197107	-0.016196	2.185495
81.533508	1495.731796	5.202112	-0.016289	2.190767
81.832039	1503.856184	5.207117	-0.016350	2.196036
82.015715	1511.914067	5.212122	-0.016389	2.201239
82.283168	1520.010501	5.217126	-0.016445	2.206461
82.590108	1528.086853	5.222131	-0.016507	2.211663
82.810756	1536.174538	5.227136	-0.016554	2.216851
83.371641	1544.221297	5.232141	-0.016664	2.222031
83.617513	1552.300973	5.237146	-0.016715	2.227192
84.034473	1560.397783	5.242150	-0.016798	2.232368
84.037211	1568.509431	5.247155	-0.016804	2.237503
84.306550	1576.568846	5.252160	-0.016860	2.242618
84.443970	1584.675930	5.257165	-0.016891	2.247739
84.801692	1592.730417	5.262170	-0.016963	2.252835
85.139851	1600.798158	5.267174	-0.017031	2.257926
85.651598	1608.840276	5.272179	-0.017132	2.263005
85.814822	1616.917896	5.277184	-0.017168	2.268064
86.161774	1625.085540	5.282189	-0.017238	2.273183
86.093985	1633.173126	5.287194	-0.017231	2.278206
86.243219	1641.230163	5.292198	-0.017264	2.283217
86.470200	1649.275108	5.297203	-0.017312	2.288216
86.707645	1657.348521	5.302208	-0.017361	2.293223
87.257417	1665.368656	5.307213	-0.017469	2.298212
87.432841	1673.433628	5.312218	-0.017507	2.303187
87.955746	1681.472592	5.317222	-0.017610	2.308163
88.425388	1689.553419	5.322227	-0.017703	2.313151
88.548721	1697.633901	5.327232	-0.017731	2.318098
88.972187	1705.681276	5.332237	-0.017816	2.323040
89.374449	1713.744613	5.337242	-0.017896	2.327978
89.708739	1721.843368	5.342246	-0.017964	2.332923
89.998036	1729.911748	5.347251	-0.018023	2.337834
90.484745	1737.945946	5.352256	-0.018119	2.342731
90.880578	1746.038368	5.357261	-0.018198	2.347645
91.054316	1754.143308	5.362266	-0.018236	2.352538
91.337882	1762.219191	5.367270	-0.018294	2.357412
91.635324	1770.260070	5.372275	-0.018355	2.362257
91.870520	1778.321093	5.377280	-0.018404	2.367098
92.332156	1786.378259	5.382285	-0.018496	2.371946
92.668435	1794.442323	5.387290	-0.018564	2.376777
93.100592	1802.484147	5.392294	-0.018650	2.381593
93.233859	1810.587602	5.397299	-0.018680	2.386412
93.666431	1818.636353	5.402304	-0.018766	2.391212
94.001866	1826.718784	5.407309	-0.018834	2.396016
93.961100	1834.793410	5.412314	-0.018832	2.400775
94.353456	1842.833246	5.417318	-0.018910	2.405538
94.440275	1850.921417	5.422323	-0.018932	2.410296
94.764405	1858.998384	5.427328	-0.018998	2.415057
95.118198	1867.056600	5.432333	-0.019069	2.419800
95.556817	1875.087794	5.437338	-0.019156	2.424524
95.841435	1883.177296	5.442342	-0.019215	2.429261
95.929607	1891.348748	5.447347	-0.019237	2.434021
96.236538	1899.356167	5.452352	-0.019299	2.438693
96.654975	1907.377144	5.457357	-0.019383	2.443373
96.488053	1915.464251	5.462362	-0.019357	2.448037
97.000388	1923.497558	5.467366	-0.019458	2.452713
97.263231	1931.554555	5.472371	-0.019512	2.457375
97.266149	1939.616756	5.477376	-0.019518	2.462011
97.662018	1947.670859	5.482381	-0.019597	2.466664
97.809650	1955.734364	5.487386	-0.019630	2.471294
98.161566	1963.786208	5.492390	-0.019701	2.475924
98.376233	1971.840826	5.497395	-0.019747	2.480537
98.657184	1979.873997	5.502400	-0.019804	2.485134
99.032546	1987.931694	5.507405	-0.019880	2.489744
99.033222	1996.024463	5.512410	-0.019885	2.494337
99.536522	2004.054755	5.517414	-0.019984	2.498923
99.762753	2012.120978	5.522419	-0.020032	2.503500
100.066696	2020.155282	5.527424	-0.020094	2.508057
100.130698	2028.302674	5.532429	-0.020112	2.512652
100.533323	2036.308986	5.537434	-0.020192	2.517184
100.902537	2044.332604	5.542438	-0.020266	2.521714
101.065570	2052.416271	5.547443	-0.020302	2.526256
101.264066	2060.455588	5.552448	-0.020344	2.530766
101.552606	2068.539854	5.557453	-0.020403	2.535301
101.631866	2076.586980	5.562458	-0.020424	2.539791
102.078657	2084.590929	5.567462	-0.020512	2.544276
102.684132	2092.643124	5.572467	-0.020630	2.548790
102.799622	2100.728503	5.577472	-0.020657	2.553281
103.016983	2108.798908	5.582477	-0.020703	2.557762
103.243156	2116.829607	5.587482	-0.020751	2.562214
103.581729	2124.880049	5.592486	-0.020819	2.566677
103.854925	2132.929981	5.597491	-0.020876	2.571128
104.227517	2140.987769	5.602496	-0.020951	2.575581
104.606271	2149.051277	5.607501	-0.021027	2.580031
104.810149	2157.082154	5.612506	-0.021070	2.584443
104.924403	2165.179850	5.617510	-0.021097	2.588878
105.366243	2173.370734	5.622515	-0.021184	2.593378
105.653390	2181.390706	5.627520	-0.021243	2.597767
105.691675	2189.434226	5.632525	-0.021256	2.602145
105.884564	2197.434652	5.637530	-0.021297	2.606502
106.223073	2205.462175	5.642534	-0.021366	2.610876
106.636991	2213.509307	5.647539	-0.021448	2.615258
106.549638	2221.546477	5.652544	-0.021437	2.619595
107.001526	2229.568671	5.657549	-0.021527	2.623951
107.118121	2237.629973	5.662554	-0.021554	2.628300
107.560916	2245.690305	5.667558	-0.021642	2.632662
107.897440	2253.734582	5.672563	-0.021710	2.637001
108.124810	2261.771341	5.677568	-0.021758	2.641322
108.449725	2269.816721	5.682573	-0.021824	2.645647
108.460684	2277.875654	5.687578	-0.021831	2.649951
108.900850	2285.938510	5.692582	-0.021919	2.654279
109.197350	2293.977180	5.697587	-0.021979	2.658577
109.410267	2302.015139	5.702592	-0.022024	2.662862
109.573334	2310.085212	5.707597	-0.022060	2.667154
109.969431	2318.115259	5.712602	-0.022139	2.671433
110.324879	2326.198220	5.717606	-0.022211	2.675730
110.643350	2334.205968	5.722611	-0.022276	2.679979
110.876671	2342.200181	5.727616	-0.022325	2.684208
110.839921	2350.315786	5.732621	-0.022323	2.688477
111.129587	2358.342444	5.737626	-0.022383	2.692713
111.523758	2366.409822	5.742630	-0.022462	2.696971
111.738440	2374.441397	5.747635	-0.022507	2.701191
111.633326	2382.504367	5.752640	-0.022493	2.705402
111.942487	2390.537342	5.757645	-0.022556	2.709616
112.120870	2398.606459	5.762650	-0.022595	2.713834
112.464674	2406.629455	5.767654	-0.022664	2.718032
112.835635	2414.651599	5.772659	-0.022738	2.722224
113.287823	2422.659195	5.777664	-0.022828	2.726408
113.244492	2430.761215	5.782669	-0.022825	2.730603
113.497464	2438.822374	5.787674	-0.022878	2.734789
113.772051	2446.849320	5.792678	-0.022935	2.738952
114.038732	2454.889580	5.797683	-0.022990	2.743115
114.022568	2462.954406	5.802688	-0.022992	2.747268
114.661147	2471.021027	5.807693	-0.023116	2.751454
114.809913	2479.105054	5.812698	-0.023150	2.755614
115.226845	2487.095501	5.817702	-0.023233	2.759735
115.347082	2495.145784	5.822707	-0.023261	2.763863
115.563930	2503.157122	5.827712	-0.023306	2.767971
116.014144	2511.204613	5.832717	-0.023396	2.772104
116.015487	2519.278796	5.837722	-0.023401	2.776219
116.254027	2527.312745	5.842726	-0.023451	2.780321
116.395619	2535.335551	5.847731	-0.023483	2.784406
116.433866	2543.397632	5.852736	-0.023496	2.788498
116.679012	2551.464233	5.857741	-0.023547	2.792599
116.938323	2559.488078	5.862746	-0.023600	2.796672
117.297123	2567.504230	5.867750	-0.023673	2.800742
117.555551	2575.518440	5.872755	-0.023726	2.804799
117.750617	2583.577763	5.877760	-0.023768	2.808870
118.136773	2591.637470	5.882765	-0.023845	2.812945
118.302990	2599.660934	5.887770	-0.023882	2.816984
118.633831	2607.693336	5.892774	-0.023949	2.821030
118.878442	2615.744215	5.897779	-0.024000	2.825076
118.936200	2623.796885	5.902784	-0.024016	2.829105
119.030112	2631.928290	5.907789	-0.024039	2.833170
119.410859	2639.931611	5.912794	-0.024115	2.837182
119.612599	2647.951766	5.917798	-0.024158	2.841186
119.740340	2655.994896	5.922803	-0.024187	2.845192
119.657176	2664.029281	5.927808	-0.024177	2.849176
119.954706	2672.091687	5.932813	-0.024238	2.853190
120.269911	2680.104300	5.937818	-0.024302	2.857174
120.849063	2688.109905	5.942822	-0.024415	2.861164
121.176347	2696.144589	5.947827	-0.024482	2.865149
121.226677	2704.197671	5.952832	-0.024497	2.869121
121.673113	2712.276559	5.957837	-0.024585	2.873123
121.703855	2720.304817	5.962842	-0.024596	2.877072
121.857892	2728.342443	5.967846	-0.024631	2.881026
122.091987	2736.396294	5.972851	-0.024680	2.884987
122.357482	2744.401059	5.977856	-0.024734	2.888920
122.716715	2752.458228	5.982861	-0.024807	2.892879
122.552814	2760.543086	5.987866	-0.024782	2.896818
122.844454	2768.551887	5.992870	-0.024841	2.900738
123.067267	2776.584433	5.997875	-0.024888	2.904661
123.096241	2784.619805	6.002880	-0.024899	2.908570
123.661203	2792.708611	6.007885	-0.025010	2.912528
123.875781	2800.747410	6.012890	-0.025055	2.916438
124.143712	2808.767393	6.017894	-0.025111	2.920336
124.467133	2816.756633	6.022899	-0.025176	2.924217
124.677845	2824.784522	6.027904	-0.025221	2.928105
124.936666	2832.858755	6.032909	-0.025275	2.932013
124.880720	2840.919847	6.037914	-0.025270	2.935894
124.893156	2848.949721	6.042918	-0.025277	2.939757
125.097419	2856.956332	6.047923	-0.025321	2.943614
125.371212	2864.970580	6.052928	-0.025377	2.947474
125.832871	2873.030575	6.057933	-0.025469	2.951360
126.094597	2881.064289	6.062938	-0.025523	2.955217
126.235072	2889.088382	6.067942	-0.025554	2.959059
126.467083	2897.138662	6.072947	-0.025603	2.962914
127.031622	2905.127778	6.077952	-0.025713	2.966750
127.570447	2913.169023	6.082957	-0.025819	2.970606
127.678708	2921.253958	6.087962	-0.025845	2.974455
127.818292	2929.285548	6.092966	-0.025876	2.978275
128.190387	2937.320522	6.097971	-0.025951	2.982104
128.424630	2945.335844	6.102976	-0.026000	2.985912
128.568748	2953.396866	6.107981	-0.026032	2.989732
128.666278	2961.467271	6.112986	-0.026056	2.993548
128.815989	2969.506089	6.117990	-0.026089	2.997348
129.135931	2977.501397	6.122995	-0.026154	3.001131
129.274479	2985.499547	6.128000	-0.026185	3.004902
129.607546	2993.581069	6.133005	-0.026253	3.008716
129.832257	3001.606545	6.138010	-0.026300	3.012494
130.258382	3009.646415	6.143014	-0.026385	3.016284
130.606404	3017.665436	6.148019	-0.026455	3.020055
130.704167	3025.680740	6.153024	-0.026479	3.023808
131.035599	3033.757942	6.158029	-0.026546	3.027596
131.422749	3041.780699	6.163034	-0.026624	3.031357
131.568606	3049.864860	6.168038	-0.026656	3.035130
131.583607	3057.895520	6.173043	-0.026664	3.038867
131.614309	3065.908910	6.178048	-0.026675	3.042592
132.127914	3073.932720	6.183053	-0.026777	3.046341
132.385860	3081.949927	6.188058	-0.026830	3.050069
132.614260	3090.032759	6.193062	-0.026878	3.053822
132.944361	3098.059810	6.198067	-0.026945	3.057550
133.149468	3106.079891	6.203072	-0.026989	3.061263
133.213580	3114.124934	6.208077	-0.027006	3.064977
133.509151	3122.152059	6.213082	-0.027066	3.068689
133.616515	3130.242202	6.218086	-0.027092	3.072417
133.798921	3138.329836	6.223091	-0.027131	3.076142
134.126973	3146.264901	6.228096	-0.027198	3.079800
134.525170	3154.256289	6.233101	-0.027277	3.083482
134.499605	3162.320109	6.238106	-0.027278	3.087174
134.540917	3170.351987	6.243110	-0.027291	3.090849
134.929136	3178.368740	6.248115	-0.027369	3.094530
135.112922	3186.398695	6.253120	-0.027408	3.098202
135.373192	3194.444307	6.258125	-0.027462	3.101881
135.646395	3202.455080	6.263130	-0.027519	3.105540
135.690120	3210.490157	6.268134	-0.027532	3.109195
135.948368	3218.566957	6.273139	-0.027586	3.112875
136.009351	3226.618701	6.278144	-0.027603	3.116529
136.410366	3234.606129	6.283149	-0.027683	3.120166
136.772818	3242.574468	6.288154	-0.027755	3.123788
136.865814	3250.652889	6.293158	-0.027778	3.127444
137.116365	3258.698255	6.298163	-0.027830	3.131087
137.211821	3266.758730	6.303168	-0.027854	3.134726
137.525991	3274.801542	6.308173	-0.027918	3.138363
137.566837	3282.813356	6.313178	-0.027931	3.141969
137.750847	3290.846778	6.318182	-0.027970	3.145587
137.959680	3298.880160	6.323187	-0.028015	3.149202
138.291212	3306.935981	6.328192	-0.028082	3.152828
138.563069	3314.983352	6.333197	-0.028138	3.156444
138.950935	3322.954779	6.338202	-0.028215	3.160026
138.978294	3330.972558	6.343206	-0.028226	3.163610
139.375308	3339.014022	6.348211	-0.028305	3.167216
139.318062	3347.064644	6.353216	-0.028300	3.170802
139.584787	3355.137287	6.358221	-0.028355	3.174408
139.915038	3363.117609	6.363226	-0.028422	3.177971
140.241607	3371.139759	6.368230	-0.028488	3.181549
140.428479	3379.171137	6.373235	-0.028529	3.185121
140.618837	3387.213411	6.378240	-0.028569	3.188694
140.926071	3395.265635	6.383245	-0.028632	3.192272
141.069155	3403.329991	6.388250	-0.028664	3.195845
141.220291	3411.294494	6.393254	-0.028698	3.199369
141.810140	3419.323891	6.398259	-0.028813	3.202937
142.279941	3427.344152	6.403264	-0.028906	3.206492
142.509451	3435.390603	6.408269	-0.028954	3.210044
142.553440	3443.455074	6.413274	-0.028968	3.213593
143.009476	3451.471193	6.418278	-0.029058	3.217133
143.155996	3459.526888	6.423283	-0.029091	3.220674
143.442388	3467.500731	6.428288	-0.029149	3.224181
143.761623	3475.544538	6.433293	-0.029214	3.227716
144.172231	3483.601651	6.438298	-0.029296	3.231257
144.271993	3491.708225	6.443302	-0.029320	3.234802
144.247591	3499.727928	6.448307	-0.029321	3.238301
144.517627	3507.681679	6.453312	-0.029377	3.241779
144.909506	3515.693082	6.458317	-0.029455	3.245284
145.134117	3523.705824	6.463322	-0.029502	3.248778
145.410778	3531.746234	6.468326	-0.029559	3.252283
145.665832	3539.807525	6.473331	-0.029612	3.255792
145.661994	3547.816407	6.478336	-0.029617	3.259264
145.865272	3555.872553	6.483341	-0.029660	3.262762
146.063051	3563.886690	6.488346	-0.029703	3.266237
146.128310	3571.907103	6.493350	-0.029720	3.269706
146.398495	3579.994108	6.498355	-0.029776	3.273208
146.674594	3587.985798	6.503360	-0.029833	3.276665
146.832627	3596.012001	6.508365	-0.029868	3.280129
146.988789	3604.030247	6.513370	-0.029902	3.283585
147.317559	3612.018190	6.518374	-0.029969	3.287032
147.630850	3620.080089	6.523379	-0.030033	3.290506
147.547250	3628.149209	6.528384	-0.030022	3.293964
147.883908	3636.162838	6.533389	-0.030091	3.297411
148.022901	3644.191039	6.538394	-0.030122	3.300853
148.189092	3652.184359	6.543398	-0.030158	3.304278
148.443677	3660.237411	6.548403	-0.030211	3.307728
148.492266	3668.267543	6.553408	-0.030226	3.311156
148.942625	3676.322407	6.558413	-0.030315	3.314607
148.795268	3684.373523	6.563418	-0.030293	3.318030
149.060707	3692.375865	6.568422	-0.030348	3.321444
149.467541	3700.369702	6.573427	-0.030429	3.324857
149.501759	3708.407668	6.578432	-0.030441	3.328270
149.761537	3716.462843	6.583437	-0.030494	3.331696
150.046096	3724.503626	6.588442	-0.030553	3.335113
150.247801	3732.500254	6.593446	-0.030596	3.338505
150.427274	3740.549907	6.598451	-0.030635	3.341915
150.587148	3748.528965	6.603456	-0.030670	3.345290
150.886755	3756.563267	6.608461	-0.030731	3.348691
150.929984	3764.646613	6.613466	-0.030745	3.352100
151.223493	3772.656504	6.618470	-0.030805	3.355483
151.706293	3780.656826	6.623475	-0.030900	3.358866
151.784567	3788.671248	6.628480	-0.030920	3.362236
151.899178	3796.715938	6.633485	-0.030947	3.365618
152.118783	3804.718079	6.638490	-0.030993	3.368981
152.237348	3812.807792	6.643494	-0.031021	3.372374
152.430452	3820.866526	6.648499	-0.031062	3.375754
152.670818	3828.835281	6.653504	-0.031112	3.379094
153.020745	3836.845374	6.658509	-0.031183	3.382452
153.127273	3844.897676	6.663514	-0.031208	3.385816
153.354079	3852.885691	6.668518	-0.031256	3.389154
153.688959	3861.021860	6.673523	-0.031324	3.392554
153.998706	3869.063351	6.678528	-0.031387	3.395910
154.044211	3877.031389	6.683533	-0.031401	3.399223
154.382656	3885.024852	6.688538	-0.031469	3.402553
154.551501	3893.049507	6.693542	-0.031506	3.405888
154.734806	3901.074877	6.698547	-0.031545	3.409219
155.084797	3909.081518	6.703552	-0.031616	3.412546
155.266181	3917.161477	6.708557	-0.031655	3.415894
155.208124	3925.152069	6.713562	-0.031650	3.419193
155.360379	3933.152685	6.718566	-0.031684	3.422500
155.605026	3941.219419	6.723571	-0.031735	3.425835
155.766267	3949.212268	6.728576	-0.031770	3.429133
155.950223	3957.305907	6.733581	-0.031810	3.432470
156.292278	3965.338379	6.738586	-0.031879	3.435784
156.448939	3973.330009	6.743590	-0.031913	3.439072
156.579398	3981.371078	6.748595	-0.031943	3.442376
156.713666	3989.364775	6.753600	-0.031974	3.445658
157.020638	3997.405570	6.758605	-0.032036	3.448961
157.043659	4005.442799	6.763610	-0.032046	3.452250
157.188796	4013.500799	6.768614	-0.032078	3.455549
157.696168	4021.497696	6.773619	-0.032178	3.458831
157.879302	4029.523065	6.778624	-0.032218	3.462112
158.258349	4037.514417	6.783629	-0.032294	3.465381
158.476321	4045.560099	6.788634	-0.032340	3.468665
158.610053	4053.605628	6.793638	-0.032370	3.471942
158.793752	4061.701742	6.798643	-0.032410	3.475239
159.034161	4069.631916	6.803648	-0.032460	3.478467
159.255375	4077.683502	6.808653	-0.032507	3.481740
159.355670	4085.671381	6.813658	-0.032531	3.484981
159.313271	4093.698021	6.818662	-0.032528	3.488230
159.582583	4101.768691	6.823667	-0.032584	3.491503
159.750092	4109.759968	6.828672	-0.032620	3.494738
159.937972	4117.798918	6.833677	-0.032661	3.497990
160.100276	4125.824979	6.838682	-0.032696	3.501233
160.276480	4133.786959	6.843686	-0.032735	3.504447
160.599680	4141.862089	6.848691	-0.032800	3.507709
160.629023	4149.896932	6.853696	-0.032811	3.510942
160.953363	4157.938236	6.858701	-0.032877	3.514184
161.253093	4165.967233	6.863706	-0.032938	3.517417
161.369208	4173.933747	6.868710	-0.032965	3.520616
161.771368	4181.941810	6.873715	-0.033046	3.523838
161.968043	4189.983205	6.878720	-0.033088	3.527064
161.770832	4198.037817	6.883725	-0.033056	3.530280
162.237779	4206.087594	6.888730	-0.033149	3.533512
162.600277	4214.098896	6.893734	-0.033222	3.536722
162.684867	4222.150370	6.898739	-0.033243	3.539937
162.565445	4230.150908	6.903744	-0.033226	3.543122
162.779927	4238.186859	6.908749	-0.033271	3.546329
162.894639	4246.225101	6.913754	-0.033298	3.549530
163.217102	4254.319574	6.918758	-0.033364	3.552758
163.377368	4262.392750	6.923763	-0.033399	3.555969
163.494332	4270.304130	6.928768	-0.033426	3.559111
163.686119	4278.312349	6.933773	-0.033467	3.562292
163.813128	4286.317625	6.938778	-0.033496	3.565466
163.955575	4294.343169	6.943782	-0.033528	3.568646
164.323641	4302.391745	6.948787	-0.033602	3.571839
164.286934	4310.412544	6.953792	-0.033601	3.575006
164.508299	4318.424736	6.958797	-0.033647	3.578175
164.664133	4326.450503	6.963802	-0.033682	3.581344
164.612094	4334.431984	6.968806	-0.033678	3.584487
165.057737	4342.475595	6.973811	-0.033766	3.587666
165.318706	4350.504970	6.978816	-0.033820	3.590831
165.536315	4358.538324	6.983821	-0.033866	3.593993
165.738415	4366.579181	6.988826	-0.033909	3.597156
165.941652	4374.557053	6.993830	-0.033952	3.600290
166.319680	4382.581273	6.998835	-0.034028	3.603445
166.130351	4390.633264	7.003840	-0.033998	3.606593
166.414299	4398.646538	7.008845	-0.034057	3.609735
166.607310	4406.698162	7.013850	-0.034098	3.612888
166.735854	4414.732683	7.018854	-0.034127	3.616029
166.994639	4422.701015	7.023859	-0.034181	3.619145
167.158843	4430.745495	7.028864	-0.034217	3.622285
167.462606	4438.748744	7.033869	-0.034279	3.625411
167.628705	4446.787145	7.038874	-0.034315	3.628543
167.910032	4454.830954	7.043878	-0.034373	3.631678
168.190056	4462.906061	7.048883	-0.034431	3.634823
168.095768	4470.892774	7.053888	-0.034419	3.637920
168.330566	4478.932735	7.058893	-0.034468	3.641044
168.546965	4486.889088	7.063898	-0.034513	3.644133
168.386651	4494.948428	7.068902	-0.034489	3.647249
168.736075	4502.978785	7.073907	-0.034560	3.650364
169.141935	4511.000181	7.078912	-0.034641	3.653475
169.300783	4519.077822	7.083917	-0.034676	3.656598
169.054827	4527.096098	7.088922	-0.034635	3.659685
169.173305	4535.064703	7.093926	-0.034663	3.662760
169.644285	4543.103782	7.098931	-0.034756	3.665869
169.650182	4551.089581	7.103936	-0.034762	3.668942
169.809060	4559.158707	7.108941	-0.034797	3.672049
170.010887	4567.225360	7.113946	-0.034840	3.675153
170.286450	4575.197981	7.118950	-0.034897	3.678220
170.438071	4583.203572	7.123955	-0.034931	3.681294
170.609392	4591.179571	7.128960	-0.034968	3.684355
170.845821	4599.228938	7.133965	-0.035017	3.687443
170.960339	4607.258938	7.138970	-0.035044	3.690518
171.073181	4615.333390	7.143974	-0.035071	3.693607
171.541258	4623.363501	7.148979	-0.035163	3.696686
171.452348	4631.333085	7.153984	-0.035152	3.699725
171.722050	4639.359475	7.158989	-0.035208	3.702792
171.873147	4647.391358	7.163994	-0.035241	3.705856
171.941459	4655.430417	7.168998	-0.035259	3.708917
172.113020	4663.480145	7.174003	-0.035297	3.711983
172.265397	4671.542781	7.179008	-0.035331	3.715051
172.688030	4679.502630	7.184013	-0.035415	3.718084
172.759423	4687.536995	7.189018	-0.035433	3.721133
172.923299	4695.450956	7.194022	-0.035469	3.724137
173.232722	4703.528667	7.199027	-0.035532	3.727204
173.140575	4711.539686	7.204032	-0.035521	3.730234
173.362082	4719.608326	7.209037	-0.035567	3.733291
173.428648	4727.652148	7.214042	-0.035585	3.736331
173.729921	4735.595937	7.219046	-0.035647	3.739338
173.802210	4743.669937	7.224051	-0.035666	3.742385
173.890641	4751.649280	7.229056	-0.035687	3.745395
174.222605	4759.705302	7.234061	-0.035755	3.748436
174.140305	4767.799616	7.239066	-0.035745	3.751480
174.282089	4775.782738	7.244070	-0.035777	3.754485
174.683874	4783.804461	7.249075	-0.035857	3.757508
174.527175	4791.804030	7.254080	-0.035833	3.760508
174.767797	4799.782173	7.259085	-0.035883	3.763506
175.057753	4807.807934	7.264090	-0.035943	3.766520
175.060085	4815.835309	7.269094	-0.035949	3.769526
175.344143	4823.922062	7.274099	-0.036007	3.772559
175.546923	4831.925991	7.279104	-0.036050	3.775556
175.818265	4839.955638	7.284109	-0.036106	3.778562
175.984590	4847.962995	7.289114	-0.036143	3.781554
176.112166	4855.959845	7.294118	-0.036172	3.784540
176.381660	4863.997311	7.299123	-0.036227	3.787542
176.559812	4872.050087	7.304128	-0.036266	3.790544
176.780645	4880.101758	7.309133	-0.036312	3.793545
176.990747	4888.109302	7.314138	-0.036357	3.796527
177.199969	4896.057718	7.319142	-0.036401	3.799484
177.197490	4904.104830	7.324147	-0.036406	3.802472
177.159189	4912.117439	7.329152	-0.036405	3.805443
177.465088	4920.127946	7.334157	-0.036467	3.808418
177.635944	4928.188159	7.339162	-0.036504	3.811407
177.830305	4936.157197	7.344166	-0.036546	3.814360
178.204758	4944.236939	7.349171	-0.036621	3.817356
178.287219	4952.200585	7.354176	-0.036642	3.820300
178.486529	4960.226293	7.359181	-0.036684	3.823267
178.835183	4968.289554	7.364186	-0.036755	3.826249
178.759581	4976.266594	7.369190	-0.036746	3.829188
178.954539	4984.342010	7.374195	-0.036788	3.832166
179.056410	4992.351014	7.379200	-0.036812	3.835116
179.406003	5000.347967	7.384205	-0.036883	3.838064
179.739749	5008.366571	7.389210	-0.036950	3.841017
179.697566	5016.342879	7.394214	-0.036948	3.843945
179.943644	5024.408709	7.399219	-0.036999	3.846909
179.937154	5032.419152	7.404224	-0.037003	3.849846
180.231912	5040.461587	7.409229	-0.037064	3.852798
180.518122	5048.521039	7.414234	-0.037122	3.855754
180.521354	5056.527294	7.419238	-0.037128	3.858682
180.607363	5064.581229	7.424243	-0.037150	3.861628
180.533544	5072.557763	7.429248	-0.037141	3.864539
180.840819	5080.598198	7.434253	-0.037204	3.867480
181.066116	5088.605675	7.439258	-0.037251	3.870404
181.123645	5096.832421	7.444262	-0.037268	3.873403
181.549428	5104.846650	7.449267	-0.037352	3.876329
181.585288	5112.733605	7.454272	-0.037364	3.879199
181.701444	5120.740671	7.459277	-0.037391	3.882112
182.211670	5128.700921	7.464282	-0.037492	3.885014
182.198787	5136.700386	7.469286	-0.037495	3.887917
182.460065	5144.761023	7.474291	-0.037549	3.890846
182.450506	5152.791339	7.479296	-0.037553	3.893756
182.799344	5160.779457	7.484301	-0.037623	3.896656
183.014985	5168.798800	7.489306	-0.037669	3.899562
182.943127	5176.836675	7.494310	-0.037661	3.902467
183.430917	5184.866905	7.499315	-0.037757	3.905378
183.592630	5192.814751	7.504320	-0.037792	3.908251
183.667344	5200.907189	7.509325	-0.037812	3.911173
183.747407	5208.968192	7.514330	-0.037832	3.914080
183.954345	5216.951565	7.519334	-0.037876	3.916960
184.115522	5224.906814	7.524339	-0.037911	3.919827
184.371621	5232.961230	7.529344	-0.037965	3.922730
184.485522	5240.968997	7.534349	-0.037991	3.925610
184.720352	5249.000063	7.539354	-0.038040	3.928499
184.878338	5257.021007	7.544358	-0.038075	3.931381
184.912111	5265.077654	7.549363	-0.038087	3.934272
185.046416	5273.094268	7.554368	-0.038117	3.937147
185.039573	5281.081978	7.559373	-0.038121	3.940008
185.404122	5289.091113	7.564378	-0.038195	3.942881
185.604160	5297.096040	7.569382	-0.038237	3.945747
185.710146	5305.112382	7.574387	-0.038263	3.948614
185.767330	5313.175474	7.579392	-0.038279	3.951494
186.033981	5321.239510	7.584397	-0.038334	3.954376
186.299791	5329.243900	7.589402	-0.038389	3.957235
186.390906	5337.201304	7.594406	-0.038411	3.960072
186.553700	5345.240822	7.599411	-0.038447	3.962938
186.698653	5353.220381	7.604416	-0.038479	3.965779
186.803820	5361.234867	7.609421	-0.038504	3.968631
187.219542	5369.264106	7.614426	-0.038587	3.971490
187.278590	5377.288970	7.619430	-0.038603	3.974340
187.630147	5385.364787	7.624435	-0.038674	3.977211
187.570369	5393.356715	7.629440	-0.038669	3.980044
187.693281	5401.383664	7.634445	-0.038697	3.982889
187.988817	5409.390712	7.639450	-0.038757	3.985729
188.003140	5417.398133	7.644454	-0.038766	3.988562
188.257340	5425.478789	7.649459	-0.038818	3.991422
188.343102	5433.490896	7.654464	-0.038840	3.994254
188.438306	5441.507415	7.659469	-0.038863	3.997085
188.613180	5449.501235	7.664474	-0.038901	3.999908
188.923414	5457.515887	7.669478	-0.038964	4.002738
189.101652	5465.559176	7.674483	-0.039003	4.005574
189.081401	5473.545335	7.679488	-0.039004	4.008385
189.440984	5481.599947	7.684493	-0.039077	4.011224
189.484429	5489.655016	7.689498	-0.039090	4.014056
189.668466	5497.654411	7.694502	-0.039130	4.016868
189.844859	5505.663395	7.699507	-0.039168	4.019682
189.904813	5513.687665	7.704512	-0.039185	4.022498
190.182563	5521.705345	7.709517	-0.039242	4.025312
190.177171	5529.746499	7.714522	-0.039246	4.028128
190.275585	5537.766458	7.719526	-0.039270	4.030937
190.751832	5545.921224	7.724531	-0.039364	4.033796
190.928041	5553.870651	7.729536	-0.039402	4.036577
190.929722	5561.792008	7.734541	-0.039408	4.039344
191.179557	5569.813775	7.739546	-0.039460	4.042148
191.159686	5577.796297	7.744550	-0.039462	4.044932
191.401892	5585.826971	7.749555	-0.039512	4.047734
191.513115	5593.843740	7.754560	-0.039538	4.050528
191.456003	5601.893806	7.759565	-0.039533	4.053329
191.882128	5609.930120	7.764570	-0.039618	4.056131
191.830426	5617.901307	7.769574	-0.039614	4.058900
192.075525	5625.947454	7.774579	-0.039665	4.061699
192.143174	5633.913899	7.779584	-0.039683	4.064465
192.291317	5641.962639	7.784589	-0.039716	4.067259
192.447026	5649.968019	7.789594	-0.039750	4.070036
192.663866	5657.992684	7.794598	-0.039796	4.072818
192.812383	5666.005849	7.799603	-0.039829	4.075594
193.047362	5674.009329	7.804608	-0.039878	4.078366
193.273754	5682.033159	7.809613	-0.039926	4.081143
193.267682	5690.062781	7.814618	-0.039930	4.083916
193.343949	5698.078316	7.819622	-0.039950	4.086684
193.842861	5706.067250	7.824627	-0.040048	4.089447
193.858628	5714.159598	7.829632	-0.040057	4.092237
193.962614	5722.159750	7.834637	-0.040081	4.094994
194.400716	5730.202249	7.839642	-0.040168	4.097768
194.419080	5738.177662	7.844646	-0.040177	4.100512
194.456148	5746.205859	7.849651	-0.040189	4.103273
194.533146	5754.210685	7.854656	-0.040209	4.106024
194.689248	5762.249743	7.859661	-0.040244	4.108786
194.768270	5770.342719	7.864666	-0.040264	4.111564
194.825527	5778.336366	7.869670	-0.040280	4.114305
195.192712	5786.385728	7.874675	-0.040354	4.117068
195.275128	5794.320854	7.879680	-0.040374	4.119786
195.290347	5802.364157	7.884685	-0.040383	4.122538
195.640904	5810.340181	7.889690	-0.040453	4.125270
195.649686	5818.366193	7.894694	-0.040460	4.128013
195.885569	5826.391995	7.899699	-0.040510	4.130756
196.177985	5834.452300	7.904704	-0.040570	4.133510
196.196449	5842.473985	7.909709	-0.040579	4.136246
196.226002	5850.512511	7.914714	-0.040590	4.138986
196.467435	5858.505704	7.919718	-0.040640	4.141711
196.731990	5866.517211	7.924723	-0.040695	4.144441
196.764785	5874.527626	7.929728	-0.040706	4.147166
196.782371	5882.556730	7.934733	-0.040715	4.149895
197.436964	5890.613895	7.939738	-0.040842	4.152640
197.386346	5898.589883	7.944742	-0.040838	4.155347
197.463365	5906.592420	7.949747	-0.040858	4.158062
197.627540	5914.626709	7.954752	-0.040894	4.160788
197.839501	5922.608472	7.959757	-0.040939	4.163494
198.048758	5930.666647	7.964762	-0.040983	4.166225
198.105072	5938.690144	7.969766	-0.040999	4.168940
198.425264	5946.748824	7.974771	-0.041064	4.171668
198.630639	5954.744663	7.979776	-0.041108	4.174372
198.625719	5962.737046	7.984781	-0.041112	4.177071
198.733680	5970.746605	7.989786	-0.041138	4.179775
198.926766	5978.720637	7.994790	-0.041179	4.182466
198.915367	5986.775146	7.999795	-0.041182	4.185180
198.890037	5994.813084	8.004800	-0.041183	4.187887
199.056038	6002.819424	8.009805	-0.041220	4.190583
199.374028	6010.949615	8.014810	-0.041284	4.193321
199.364079	6018.922896	8.019814	-0.041288	4.196001
199.703870	6026.906001	8.024819	-0.041356	4.198687
199.890966	6034.937315	8.029824	-0.041397	4.201385
200.069427	6042.860574	8.034829	-0.041435	4.204045
200.522147	6050.951800	8.039834	-0.041525	4.206762
200.688445	6058.884861	8.044838	-0.041561	4.209422
201.023674	6066.966130	8.049843	-0.041629	4.212131
201.077294	6074.988540	8.054848	-0.041645	4.214816
201.465874	6082.991931	8.059853	-0.041722	4.217496
201.732783	6091.019197	8.064858	-0.041778	4.220181
201.616084	6098.990235	8.069862	-0.041761	4.222842
201.905779	6107.057105	8.074867	-0.041821	4.225537
202.232717	6115.029838	8.079872	-0.041887	4.228200
202.149148	6123.093800	8.084877	-0.041877	4.230887
202.542747	6131.145203	8.089882	-0.041956	4.233573
202.778277	6139.170816	8.094886	-0.042005	4.236247
202.644886	6147.120221	8.099891	-0.041985	4.238890
202.664469	6155.144376	8.104896	-0.041994	4.241558
202.918516	6163.088935	8.109901	-0.042047	4.244200
203.251480	6171.196215	8.114906	-0.042115	4.246896
203.306446	6179.200814	8.119910	-0.042130	4.249552
203.511174	6187.246783	8.124915	-0.042174	4.252223
203.721754	6195.267587	8.129920	-0.042218	4.254883
203.667479	6203.247961	8.134925	-0.042214	4.257526
203.634506	6211.302515	8.139930	-0.042213	4.260192
203.839283	6219.289603	8.144934	-0.042257	4.262836
204.087783	6227.314575	8.149939	-0.042308	4.265491
204.106167	6235.336605	8.154944	-0.042317	4.268141
204.317365	6243.360432	8.159949	-0.042362	4.270793
204.580126	6251.442879	8.164954	-0.042416	4.273462
204.579362	6259.449283	8.169958	-0.042422	4.276102
204.686916	6267.414255	8.174963	-0.042447	4.278728
205.302631	6275.426131	8.179968	-0.042567	4.281372
205.312745	6283.415937	8.184973	-0.042574	4.284002
205.409034	6291.492983	8.189978	-0.042598	4.286660
205.411016	6299.463457	8.194982	-0.042603	4.289280
205.655890	6307.536381	8.199987	-0.042655	4.291935
205.657950	6315.536702	8.204992	-0.042660	4.294561
205.924600	6323.533549	8.209997	-0.042715	4.297188
206.090645	6331.591176	8.215002	-0.042752	4.299831
206.132508	6339.589174	8.220006	-0.042765	4.302453
206.226514	6347.577480	8.225011	-0.042788	4.305070
206.514811	6355.647182	8.230016	-0.042847	4.307714
206.775685	6363.609962	8.235021	-0.042901	4.310321
206.670103	6371.705624	8.240026	-0.042887	4.312967
206.668360	6379.662360	8.245030	-0.042892	4.315566
207.057995	6387.656053	8.250035	-0.042970	4.318179
207.076300	6395.723484	8.255040	-0.042979	4.320812
207.184908	6403.649222	8.260045	-0.043004	4.323398
207.400944	6411.727786	8.265050	-0.043050	4.326032
207.443239	6419.722220	8.270054	-0.043063	4.328637
207.542644	6427.762450	8.275059	-0.043087	4.331255
207.602898	6435.805565	8.280064	-0.043104	4.333872
207.756083	6443.824676	8.285069	-0.043138	4.336481
207.826862	6451.802393	8.290074	-0.043156	4.339073
207.981787	6459.811024	8.295078	-0.043191	4.341675
208.488346	6467.774813	8.300083	-0.043290	4.344263
208.435377	6475.853400	8.305088	-0.043286	4.346883
208.415570	6483.888958	8.310093	-0.043288	4.349488
208.813143	6491.965163	8.315098	-0.043367	4.352107
208.919530	6500.008879	8.320102	-0.043392	4.354712
209.253320	6507.969910	8.325107	-0.043460	4.357290
209.363890	6515.948911	8.330112	-0.043486	4.359871
209.387395	6523.945029	8.335117	-0.043496	4.362456
209.378759	6531.947498	8.340122	-0.043499	4.365040
209.484724	6539.962185	8.345126	-0.043525	4.367628
209.807905	6547.997870	8.350131	-0.043590	4.370222
209.973751	6556.007530	8.355136	-0.043627	4.372806
209.958714	6563.997268	8.360141	-0.043629	4.375380
210.184015	6572.056131	8.365146	-0.043677	4.377977
210.244686	6580.054959	8.370150	-0.043693	4.380552
210.574484	6588.101240	8.375155	-0.043760	4.383142
210.816652	6596.056836	8.380160	-0.043811	4.385700
210.878936	6604.073825	8.385165	-0.043828	4.388276
210.990716	6612.163750	8.390170	-0.043854	4.390875
210.930833	6620.189468	8.395174	-0.043848	4.393450
211.181508	6628.229179	8.400179	-0.043900	4.396029
211.283339	6636.182696	8.405184	-0.043925	4.398579
211.415948	6644.204708	8.410189	-0.043955	4.401149
211.693211	6652.215426	8.415194	-0.044012	4.403715
212.008794	6660.213716	8.420198	-0.044076	4.406276
212.128560	6668.237528	8.425203	-0.044104	4.408842
212.401809	6676.317376	8.430208	-0.044160	4.411426
212.597036	6684.308457	8.435213	-0.044202	4.413979
212.679687	6692.359809	8.440218	-0.044223	4.416549
212.668964	6700.299851	8.445222	-0.044226	4.419082
212.835565	6708.363226	8.450227	-0.044262	4.421654
213.162495	6716.345666	8.455232	-0.044329	4.424199
213.144648	6724.389901	8.460237	-0.044331	4.426760
213.422285	6732.428609	8.465242	-0.044388	4.429320
213.364498	6740.476902	8.470246	-0.044383	4.431880
213.604215	6748.518742	8.475251	-0.044433	4.434437
213.685330	6756.544937	8.480256	-0.044453	4.436988
213.985099	6764.465574	8.485261	-0.044514	4.439504
214.088792	6772.538155	8.490266	-0.044539	4.442066
214.151244	6780.439746	8.495270	-0.044556	4.444573
214.346383	6788.560824	8.500275	-0.044598	4.447148
214.637696	6796.539549	8.505280	-0.044658	4.449677
214.636246	6804.562193	8.510285	-0.044663	4.452217
214.856305	6812.614267	8.515290	-0.044709	4.454765
214.748493	6820.605995	8.520294	-0.044695	4.457292
214.988793	6828.586112	8.525299	-0.044745	4.459816
214.925604	6836.635795	8.530304	-0.044738	4.462358
215.133114	6844.620575	8.535309	-0.044782	4.464880
215.370346	6852.698689	8.540314	-0.044832	4.467429
215.322026	6860.691699	8.545318	-0.044828	4.469950
215.542124	6868.747624	8.550323	-0.044875	4.472490
215.825867	6876.755966	8.555328	-0.044933	4.475013
215.733298	6884.696650	8.560333	-0.044921	4.477513
216.016491	6892.749894	8.565338	-0.044979	4.480047
216.134813	6900.737047	8.570343	-0.045007	4.482559
216.322020	6908.699211	8.575347	-0.045047	4.485062
216.429704	6916.769112	8.580352	-0.045073	4.487597
216.537104	6924.792896	8.585357	-0.045098	4.490116
216.653322	6932.850016	8.590362	-0.045125	4.492645
216.659227	6940.837085	8.595367	-0.045132	4.495149
216.796095	6948.847331	8.600371	-0.045163	4.497660
217.061244	6956.883878	8.605376	-0.045217	4.500178
217.175907	6964.838590	8.610381	-0.045244	4.502668
217.296294	6972.879559	8.615386	-0.045272	4.505184
217.574079	6980.920741	8.620391	-0.045329	4.507699
217.812067	6988.917898	8.625395	-0.045379	4.510199
217.862945	6997.020101	8.630400	-0.045394	4.512730
218.005186	7005.022112	8.635405	-0.045426	4.515228
218.394920	7013.017692	8.640410	-0.045504	4.517723
218.377563	7020.981868	8.645415	-0.045506	4.520207
218.615618	7028.974601	8.650419	-0.045556	4.522698
219.035831	7037.004628	8.655424	-0.045639	4.525200
219.001790	7045.012340	8.660429	-0.045638	4.527693
219.109717	7053.035543	8.665434	-0.045664	4.530189
219.161462	7061.069619	8.670439	-0.045679	4.532687
219.281668	7069.109727	8.675443	-0.045707	4.535186
219.343378	7077.096373	8.680448	-0.045724	4.537667
219.546373	7085.068465	8.685453	-0.045767	4.540142
219.771218	7093.115328	8.690458	-0.045814	4.542639
220.054245	7101.073734	8.695463	-0.045872	4.545107
220.018659	7109.171321	8.700467	-0.045871	4.547617
220.136076	7117.199985	8.705472	-0.045898	4.550104
220.299500	7125.190496	8.710477	-0.045934	4.552577
220.262932	7133.254015	8.715482	-0.045933	4.555072
220.420741	7141.232179	8.720487	-0.045968	4.557540
220.653195	7149.223499	8.725491	-0.046016	4.560010
220.842698	7157.262906	8.730496	-0.046057	4.562493
220.927357	7165.227288	8.735501	-0.046078	4.564952
221.115227	7173.276575	8.740506	-0.046119	4.567436
221.241599	7181.276880	8.745511	-0.046148	4.569903
221.464056	7189.302510	8.750515	-0.046194	4.572377
221.622877	7197.380437	8.755520	-0.046229	4.574866
221.505535	7205.407895	8.760525	-0.046213	4.577337
221.668874	7213.437830	8.765530	-0.046249	4.579808
221.817066	7221.394029	8.770535	-0.046282	4.582255
221.958739	7229.401296	8.775539	-0.046314	4.584717
222.172320	7237.417846	8.780544	-0.046359	4.587180
222.445950	7245.411211	8.785549	-0.046415	4.589634
222.676334	7253.492495	8.790554	-0.046464	4.592114
222.745743	7261.517433	8.795559	-0.046482	4.594576
222.809513	7269.491707	8.800563	-0.046499	4.597020
222.937334	7277.511963	8.805568	-0.046528	4.599477
222.928607	7285.547938	8.810573	-0.046532	4.601938
223.070771	7293.519715	8.815578	-0.046564	4.604378
223.056393	7301.568383	8.820583	-0.046567	4.606840
223.252890	7309.533400	8.825587	-0.046609	4.609275
223.378400	7317.615158	8.830592	-0.046638	4.611745
223.540265	7325.586774	8.835597	-0.046673	4.614179
223.961030	7333.676245	8.840602	-0.046757	4.616648
223.793380	7341.608345	8.845607	-0.046731	4.619068
223.936721	7349.722889	8.850611	-0.046763	4.621542
224.316549	7357.637046	8.855616	-0.046839	4.623954
224.433155	7365.657802	8.860621	-0.046867	4.626397
224.622515	7373.738320	8.865626	-0.046907	4.628857
224.614834	7381.744975	8.870631	-0.046911	4.631293
224.925689	7389.754245	8.875635	-0.046975	4.633729
224.898023	7397.804304	8.880640	-0.046975	4.636175
224.898750	7405.729137	8.885645	-0.046980	4.638583
225.197075	7413.815024	8.890650	-0.047041	4.641038
225.248427	7421.766879	8.895655	-0.047056	4.643451
225.420165	7429.792169	8.900659	-0.047094	4.645884
225.615168	7437.795018	8.905664	-0.047135	4.648310
225.668405	7445.806893	8.910669	-0.047151	4.650738
225.773455	7453.880886	8.915674	-0.047176	4.653182
225.718824	7461.895732	8.920679	-0.047171	4.655608
226.182146	7469.847311	8.925683	-0.047263	4.658013
226.292466	7477.845317	8.930688	-0.047289	4.660431
226.272558	7485.894579	8.935693	-0.047290	4.662863
226.397925	7493.882442	8.940698	-0.047319	4.665276
226.620241	7501.918345	8.945703	-0.047366	4.667701
226.667334	7509.956730	8.950707	-0.047380	4.670126
226.699218	7518.073815	8.955712	-0.047392	4.672574
226.867600	7526.115000	8.960717	-0.047428	4.674997
227.070391	7534.063153	8.965722	-0.047471	4.677391
227.113053	7542.005312	8.970727	-0.047485	4.679783
227.459877	7550.067320	8.975731	-0.047555	4.682208
227.710951	7557.985688	8.980736	-0.047607	4.684589
227.692509	7566.080141	8.985741	-0.047609	4.687022
227.935111	7574.083675	8.990746	-0.047660	4.689427
227.997331	7582.096563	8.995751	-0.047677	4.691833
228.013010	7590.075848	9.000755	-0.047685	4.694228
228.244403	7598.198026	9.005760	-0.047733	4.696664
228.242280	7606.076123	9.010765	-0.047738	4.699026
228.291160	7614.142983	9.015770	-0.047753	4.701443
228.242382	7622.124715	9.020775	-0.047749	4.703834
228.630243	7630.176244	9.025779	-0.047827	4.706244
228.879876	7638.169455	9.030784	-0.047879	4.708635
228.899244	7646.209976	9.035789	-0.047888	4.711039
229.252719	7654.272907	9.040794	-0.047959	4.713449
229.163809	7662.268617	9.045799	-0.047948	4.715838
229.200041	7670.266247	9.050803	-0.047960	4.718226
229.463003	7678.268810	9.055808	-0.048015	4.720613
229.842269	7686.253503	9.060813	-0.048091	4.722994
229.826567	7694.350978	9.065818	-0.048093	4.725408
229.839769	7702.334438	9.070823	-0.048101	4.727787
230.074943	7710.334456	9.075827	-0.048150	4.730169
230.197240	7718.398389	9.080832	-0.048178	4.732570
230.159237	7726.370477	9.085837	-0.048177	4.734942
230.258022	7734.445551	9.090842	-0.048201	4.737343
230.427683	7742.405704	9.095847	-0.048238	4.739708
230.554034	7750.456711	9.100851	-0.048266	4.742100
230.743276	7758.480941	9.105856	-0.048307	4.744482
230.953606	7766.475836	9.110861	-0.048352	4.746854
231.196832	7774.450959	9.115866	-0.048402	4.749219
231.219969	7782.529919	9.120871	-0.048412	4.751614
231.371609	7790.503754	9.125875	-0.048446	4.753977
231.700917	7798.562709	9.130880	-0.048513	4.756362
231.787981	7806.505963	9.135885	-0.048534	4.758714
231.883110	7814.577819	9.140890	-0.048557	4.761102
232.091332	7822.561141	9.145895	-0.048602	4.763462
232.085063	7830.545913	9.150899	-0.048606	4.765822
232.319412	7838.602086	9.155904	-0.048655	4.768201
232.417636	7846.545411	9.160909	-0.048678	4.770547
232.647209	7854.663644	9.165914	-0.048727	4.772942
232.561498	7862.621085	9.170919	-0.048716	4.775290
232.751927	7870.650634	9.175923	-0.048757	4.777656
232.928856	7878.637443	9.180928	-0.048795	4.780009
232.916057	7886.661753	9.185933	-0.048798	4.782373
233.262409	7894.686459	9.190938	-0.048868	4.784734
233.110171	7902.691379	9.195943	-0.048845	4.787090
233.311414	7910.670124	9.200947	-0.048888	4.789436
233.606050	7918.777420	9.205952	-0.048949	4.791818
233.734916	7926.783385	9.210957	-0.048978	4.794170
233.932289	7934.804976	9.215962	-0.049020	4.796525
233.668075	7942.721616	9.220967	-0.048976	4.798850
234.012936	7950.798037	9.225971	-0.049046	4.801218
234.168875	7958.778805	9.230976	-0.049080	4.803558
234.124612	7966.825436	9.235981	-0.049078	4.805916
234.233578	7974.828303	9.240986	-0.049103	4.808260
234.409173	7982.859641	9.245991	-0.049142	4.810611
234.446200	7990.255782	9.250995	-0.049153	4.812776
234.406303	7994.824499	9.256000	-0.049149	4.814113

234.661244	7997.214116	9.261005	-0.049198	4.814810
235.069089	7998.530504	9.266010	-0.049275	4.815193
234.819643	7998.986583	9.271015	-0.049229	4.815328
234.843524	7999.801536	9.276019	-0.049235	4.815566
235.165713	7999.819590	9.281024	-0.049295	4.815570
235.036582	7999.800431	9.286029	-0.049271	4.815565
235.077375	7999.840611	9.291034	-0.049279	4.815577
235.253220	7999.858427	9.296039	-0.049312	4.815581
235.204569	7999.876871	9.301043	-0.049303	4.815587
235.191576	7999.872408	9.306048	-0.049301	4.815585
235.268360	7999.854453	9.311053	-0.049315	4.815580
235.563861	7999.877414	9.316058	-0.049370	4.815585
235.421545	7999.830283	9.321063	-0.049344	4.815572
235.270996	7999.852413	9.326067	-0.049316	4.815579
235.453305	7999.857523	9.331072	-0.049350	4.815580
235.430024	7999.850757	9.336077	-0.049346	4.815578
235.507298	7999.879785	9.341082	-0.049361	4.815586
235.591218	7999.836324	9.346087	-0.049377	4.815573
235.696148	7999.860464	9.351091	-0.049396	4.815579
235.755971	7999.830491	9.356096	-0.049408	4.815570
235.729397	7999.843956	9.361101	-0.049403	4.815574
235.908461	7999.877839	9.366106	-0.049437	4.815583
235.736243	7999.855845	9.371111	-0.049405	4.815578
235.890862	7999.853033	9.376115	-0.049434	4.815576
236.080782	7999.868943	9.381120	-0.049469	4.815580
235.838817	7999.849020	9.386125	-0.049424	4.815575
236.009824	7999.887044	9.391130	-0.049456	4.815586
236.040344	7999.875812	9.396135	-0.049462	4.815582
235.965717	7999.868213	9.401139	-0.049449	4.815580
236.156423	7999.891610	9.406144	-0.049484	4.815586
236.262880	7999.876272	9.411149	-0.049504	4.815581
236.329515	7999.906197	9.416154	-0.049517	4.815590
236.183928	7999.850470	9.421159	-0.049490	4.815574
235.962966	7999.855443	9.426163	-0.049449	4.815577
236.112008	7999.858946	9.431168	-0.049477	4.815577
236.095501	7999.848019	9.436173	-0.049474	4.815574
236.147338	7999.884109	9.441178	-0.049484	4.815584
236.296080	7999.868391	9.446183	-0.049512	4.815579
236.355424	7999.870439	9.451187	-0.049523	4.815579
236.246008	7999.884695	9.456192	-0.049503	4.815584
236.370212	7999.866443	9.461197	-0.049526	4.815578
236.443062	7999.871913	9.466202	-0.049540	4.815579
236.347571	7999.867178	9.471207	-0.049522	4.815578
236.249596	7999.883754	9.476211	-0.049504	4.815583
236.548072	7999.887548	9.481216	-0.049560	4.815583
236.543114	7999.870403	9.486221	-0.049559	4.815578
236.458563	7999.906415	9.491226	-0.049544	4.815589
236.546177	7999.915328	9.496231	-0.049560	4.815591
236.665104	7999.892720	9.501235	-0.049583	4.815584
236.646250	7999.908446	9.506240	-0.049579	4.815589
236.518029	7999.913855	9.511245	-0.049556	4.815591
236.848966	7999.902162	9.516250	-0.049618	4.815586
236.725056	7999.903371	9.521255	-0.049595	4.815587
236.478758	7999.871632	9.526259	-0.049549	4.815579
236.617740	7999.897393	9.531264	-0.049575	4.815586
236.552275	7999.877130	9.536269	-0.049563	4.815580
236.659181	7999.905573	9.541274	-0.049583	4.815588
236.685618	7999.900681	9.546279	-0.049588	4.815586
236.662333	7999.887509	9.551283	-0.049584	4.815582
236.832872	7999.879618	9.556288	-0.049616	4.815579
236.957749	7999.870986	9.561293	-0.049640	4.815576
236.805161	7999.892015	9.566298	-0.049611	4.815583
237.005451	7999.879269	9.571303	-0.049649	4.815578
236.969035	7999.905386	9.576307	-0.049642	4.815586
236.950832	7999.892296	9.581312	-0.049639	4.815582
236.846550	7999.861794	9.586317	-0.049620	4.815574
236.951765	7999.887007	9.591322	-0.049640	4.815581
236.980515	7999.872544	9.596327	-0.049645	4.815577
236.964618	7999.859491	9.601331	-0.049642	4.815573
236.999490	7999.892104	9.606336	-0.049649	4.815582
236.695514	7999.864766	9.611341	-0.049593	4.815576
236.876307	7999.883733	9.616346	-0.049627	4.815580
237.257827	7999.866456	9.621351	-0.049698	4.815573
237.181524	7999.873776	9.626355	-0.049684	4.815576
237.223944	7999.883023	9.631360	-0.049692	4.815578
237.013180	7999.878551	9.636365	-0.049653	4.815578
236.965765	7999.888474	9.641370	-0.049644	4.815581
236.997007	7999.843090	9.646375	-0.049650	4.815568
237.265570	7999.882700	9.651379	-0.049700	4.815578
237.233412	7999.874721	9.656384	-0.049695	4.815576
237.136896	7999.885984	9.661389	-0.049677	4.815580
237.275018	7999.895717	9.666394	-0.049703	4.815582
237.185107	7999.883598	9.671399	-0.049686	4.815579
237.270746	7999.895682	9.676403	-0.049702	4.815582
237.327852	7999.930792	9.681408	-0.049713	4.815592
237.328541	7999.872099	9.686413	-0.049714	4.815575
237.387353	7999.906168	9.691418	-0.049725	4.815584
237.175010	7999.873911	9.696423	-0.049685	4.815576
237.188562	7999.867743	9.701427	-0.049688	4.815574
237.266259	7999.873292	9.706432	-0.049703	4.815575
237.125724	7999.878501	9.711437	-0.049677	4.815577
237.223750	7999.936695	9.716442	-0.049695	4.815594
237.359218	7999.888732	9.721447	-0.049721	4.815579
237.324777	7999.881785	9.726451	-0.049714	4.815577
237.262082	7999.908543	9.731456	-0.049703	4.815586
237.239414	7999.868689	9.736461	-0.049699	4.815574
237.403194	7999.905530	9.741466	-0.049730	4.815584
237.457224	7999.884004	9.746471	-0.049740	4.815577
237.524090	7999.892581	9.751475	-0.049753	4.815580
237.382620	7999.895639	9.756480	-0.049726	4.815581
237.153559	7999.849231	9.761485	-0.049684	4.815569
237.116331	7999.875335	9.766490	-0.049677	4.815577
237.220116	7999.904797	9.771495	-0.049697	4.815585
237.340499	7999.892889	9.776499	-0.049719	4.815581
237.262384	7999.878826	9.781504	-0.049705	4.815577
237.306684	7999.890239	9.786509	-0.049713	4.815580
237.340826	7999.914299	9.791514	-0.049720	4.815587
237.395425	7999.872497	9.796519	-0.049730	4.815574
237.210232	7999.874845	9.801523	-0.049696	4.815576
237.545852	7999.887786	9.806528	-0.049759	4.815578
237.389282	7999.893802	9.811533	-0.049730	4.815581
237.601526	7999.916483	9.816538	-0.049770	4.815586
237.489362	7999.877311	9.821543	-0.049749	4.815575
237.544676	7999.900647	9.826547	-0.049759	4.815582
237.297944	7999.918011	9.831552	-0.049714	4.815588
237.309766	7999.889394	9.836557	-0.049716	4.815580
237.541972	7999.912400	9.841562	-0.049759	4.815585
237.585707	7999.920601	9.846567	-0.049768	4.815587
237.500459	7999.893610	9.851571	-0.049752	4.815580
237.404789	7999.887803	9.856576	-0.049735	4.815579
237.504783	7999.870226	9.861581	-0.049753	4.815573
237.600189	7999.943326	9.866586	-0.049771	4.815594
237.487831	7999.929774	9.871591	-0.049751	4.815591
237.424709	7999.898872	9.876595	-0.049739	4.815582
237.520747	7999.933546	9.881600	-0.049757	4.815592
237.297846	7999.886170	9.886605	-0.049716	4.815579
237.619540	7999.903155	9.891610	-0.049776	4.815582
237.495012	7999.878729	9.896615	-0.049753	4.815576
237.430610	7999.876633	9.901619	-0.049741	4.815575
237.490538	7999.891503	9.906624	-0.049752	4.815579
237.591639	7999.894230	9.911629	-0.049771	4.815580
237.706476	7999.909991	9.916634	-0.049793	4.815584
237.707131	7999.883328	9.921639	-0.049793	4.815576
237.674438	7999.878543	9.926643	-0.049787	4.815575
237.610126	7999.895667	9.931648	-0.049776	4.815580
237.806902	7999.898879	9.936653	-0.049813	4.815580
237.852856	7999.909252	9.941658	-0.049821	4.815583
237.683247	7999.883026	9.946663	-0.049790	4.815576
237.676032	7999.896806	9.951667	-0.049789	4.815580
237.685535	7999.872421	9.956672	-0.049791	4.815573
237.634205	7999.855590	9.961677	-0.049781	4.815568
237.817647	7999.895954	9.966682	-0.049816	4.815579
237.673498	7999.886157	9.971687	-0.049789	4.815577
237.725611	7999.888088	9.976691	-0.049799	4.815577
237.780876	7999.902883	9.981696	-0.049810	4.815581
237.711709	7999.869747	9.986701	-0.049797	4.815572
237.931902	7999.911776	9.991706	-0.049838	4.815583
237.980835	7999.909385	9.996711	-0.049847	4.815582
237.741523	7999.879892	10.001715	-0.049803	4.815575
237.873893	7999.931171	10.006720	-0.049828	4.815589
237.928260	7999.910718	10.011725	-0.049838	4.815583
237.788710	7999.934093	10.016730	-0.049812	4.815590
237.917442	7999.924457	10.021735	-0.049837	4.815587
238.066776	7999.911952	10.026739	-0.049865	4.815582
237.977213	7999.897703	10.031744	-0.049848	4.815579
237.925838	7999.893682	10.036749	-0.049839	4.815578
238.015365	7999.910101	10.041754	-0.049856	4.815582
238.036704	7999.886976	10.046759	-0.049860	4.815575
237.994584	7999.918340	10.051763	-0.049852	4.815585
238.029603	7999.931738	10.056768	-0.049859	4.815588
238.072888	7999.903631	10.061773	-0.049867	4.815580
237.873082	7999.927095	10.066778	-0.049830	4.815588
237.726197	7999.905508	10.071783	-0.049803	4.815582
237.703271	7999.887003	10.076787	-0.049799	4.815577
237.742047	7999.927153	10.081792	-0.049806	4.815588
237.524311	7999.886266	10.086797	-0.049766	4.815577
237.680770	7999.918719	10.091802	-0.049795	4.815586
237.913518	7999.891554	10.096807	-0.049839	4.815577
238.051191	7999.909822	10.101811	-0.049865	4.815582
238.038026	7999.924573	10.106816	-0.049862	4.815586
238.331491	7999.893056	10.111821	-0.049917	4.815576
238.160127	7999.911644	10.116826	-0.049885	4.815582
238.075935	7999.882534	10.121831	-0.049870	4.815574
238.062859	7999.894083	10.126835	-0.049868	4.815577
238.213155	7999.936046	10.131840	-0.049896	4.815589
238.100225	7999.913943	10.136845	-0.049875	4.815583
238.119484	7999.923882	10.141850	-0.049879	4.815586
238.184925	7999.928165	10.146855	-0.049891	4.815587
238.021008	7999.907369	10.151859	-0.049861	4.815581
238.041087	7999.952555	10.156864	-0.049865	4.815594
237.931202	7999.890998	10.161869	-0.049845	4.815577
237.959964	7999.903227	10.166874	-0.049850	4.815580
238.099103	7999.884150	10.171879	-0.049876	4.815574
238.194644	7999.896396	10.176883	-0.049894	4.815577
238.246488	7999.915406	10.181888	-0.049904	4.815582
237.983094	7999.887656	10.186893	-0.049855	4.815576
238.088489	7999.898994	10.191898	-0.049875	4.815578
238.199414	7999.894407	10.196903	-0.049896	4.815577
238.073262	7999.899849	10.201907	-0.049873	4.815579
238.293866	7999.914127	10.206912	-0.049914	4.815582
238.197601	7999.891227	10.211917	-0.049896	4.815576
238.087878	7999.918289	10.216922	-0.049876	4.815584
238.022870	7999.917250	10.221927	-0.049864	4.815584
238.216630	7999.914009	10.226931	-0.049900	4.815582
238.416486	7999.927950	10.231936	-0.049938	4.815585
238.280285	7999.870235	10.236941	-0.049913	4.815569
238.425319	7999.918518	10.241946	-0.049940	4.815582
238.327785	7999.906274	10.246951	-0.049922	4.815579
238.237493	7999.898419	10.251955	-0.049905	4.815577
238.298865	7999.919719	10.256960	-0.049917	4.815583
238.284199	7999.884264	10.261965	-0.049914	4.815573
238.250552	7999.920036	10.266970	-0.049908	4.815584
238.247888	7999.898657	10.271975	-0.049908	4.815577
238.410474	7999.887435	10.276979	-0.049938	4.815573
238.513252	7999.905137	10.281984	-0.049958	4.815578
238.320635	7999.873198	10.286989	-0.049922	4.815570
238.526285	7999.901113	10.291994	-0.049961	4.815577
238.467320	7999.902308	10.296999	-0.049950	4.815577
238.371279	7999.897561	10.302003	-0.049932	4.815577
238.326981	7999.937431	10.307008	-0.049924	4.815588
238.294303	7999.876060	10.312013	-0.049918	4.815571
238.400248	7999.909828	10.317018	-0.049938	4.815580
238.238303	7999.909350	10.322023	-0.049908	4.815581
238.535851	7999.908863	10.327027	-0.049964	4.815579
238.532087	7999.932308	10.332032	-0.049963	4.815586
238.536915	7999.888629	10.337037	-0.049964	4.815573
238.406894	7999.906820	10.342042	-0.049940	4.815579
238.567335	7999.946813	10.347047	-0.049970	4.815590
238.495040	7999.954197	10.352051	-0.049957	4.815592
238.617185	7999.932709	10.357056	-0.049980	4.815586
238.564942	7999.899847	10.362061	-0.049971	4.815576
238.378264	7999.922456	10.367066	-0.049936	4.815584
238.433132	7999.885996	10.372071	-0.049946	4.815573
238.469857	7999.898354	10.377075	-0.049953	4.815576
238.555031	7999.938192	10.382080	-0.049969	4.815587
238.365003	7999.884941	10.387085	-0.049934	4.815573
238.300878	7999.908473	10.392090	-0.049923	4.815580
238.348250	7999.917801	10.397095	-0.049932	4.815582
238.493793	7999.903100	10.402099	-0.049959	4.815577
238.559836	7999.922341	10.407104	-0.049971	4.815583
238.557217	7999.903097	10.412109	-0.049971	4.815577
238.516957	7999.934491	10.417114	-0.049964	4.815587
238.252526	7999.903520	10.422119	-0.049915	4.815579
238.449868	7999.909946	10.427123	-0.049952	4.815580
238.713637	7999.971905	10.432128	-0.050001	4.815596
238.590262	7999.902653	10.437133	-0.049978	4.815577
238.604420	7999.910374	10.442138	-0.049981	4.815579
238.511819	7999.888600	10.447143	-0.049964	4.815573
238.451941	7999.866291	10.452147	-0.049953	4.815567
238.565632	7999.894848	10.457152	-0.049974	4.815575
238.669915	7999.886950	10.462157	-0.049994	4.815572
238.704918	7999.927041	10.467162	-0.050001	4.815583
238.688164	7999.904364	10.472167	-0.049998	4.815577
238.528918	7999.903929	10.477171	-0.049968	4.815577
238.729471	7999.943507	10.482176	-0.050006	4.815588
238.627666	7999.908771	10.487181	-0.049987	4.815578
238.837365	7999.917534	10.492186	-0.050026	4.815580
238.784115	7999.917754	10.497191	-0.050017	4.815580
238.729069	7999.907268	10.502195	-0.050007	4.815577
238.745783	7999.918233	10.507200	-0.050010	4.815581
238.656767	7999.905060	10.512205	-0.049994	4.815577
238.689401	7999.910946	10.517210	-0.050000	4.815579
238.724375	7999.892313	10.522215	-0.050007	4.815573
238.755187	7999.894966	10.527219	-0.050012	4.815574
238.951873	7999.938752	10.532224	-0.050049	4.815586
238.757355	7999.888630	10.537229	-0.050013	4.815572
238.559199	7999.919593	10.542234	-0.049977	4.815582
238.628011	7999.963437	10.547239	-0.049990	4.815594
238.621661	7999.939861	10.552243	-0.049989	4.815587
238.575073	7999.953002	10.557248	-0.049980	4.815592
238.559576	7999.922872	10.562253	-0.049977	4.815583
238.636842	7999.924144	10.567258	-0.049992	4.815583
238.559416	7999.922904	10.572263	-0.049978	4.815583
238.482825	7999.900323	10.577267	-0.049964	4.815577
238.593350	7999.920286	10.582272	-0.049985	4.815582
238.607635	7999.884234	10.587277	-0.049987	4.815571
238.509997	7999.909357	10.592282	-0.049969	4.815579
238.594632	7999.916088	10.597287	-0.049985	4.815581
238.774852	7999.874190	10.602291	-0.050019	4.815567
238.618626	7999.901565	10.607296	-0.049990	4.815576
238.561326	7999.876094	10.612301	-0.049980	4.815569
238.665523	7999.885278	10.617306	-0.049999	4.815571
238.701189	7999.885875	10.622311	-0.050006	4.815571
238.655813	7999.881952	10.627315	-0.049998	4.815570
238.800884	7999.919560	10.632320	-0.050025	4.815581
238.804534	7999.875861	10.637325	-0.050026	4.815568
238.917083	7999.908671	10.642330	-0.050047	4.815577
239.033353	7999.881749	10.647335	-0.050069	4.815568
238.876562	7999.883490	10.652339	-0.050040	4.815570
238.900686	7999.925539	10.657344	-0.050045	4.815582
238.927452	7999.864065	10.662349	-0.050050	4.815564
238.774097	7999.932058	10.667354	-0.050022	4.815584
238.813490	7999.915632	10.672359	-0.050029	4.815579
238.779435	7999.903352	10.677363	-0.050023	4.815576
238.918526	7999.913103	10.682368	-0.050049	4.815578
238.875403	7999.886795	10.687373	-0.050041	4.815571
238.812235	7999.913546	10.692378	-0.050030	4.815579
238.897499	7999.897865	10.697383	-0.050046	4.815574
238.884690	7999.893403	10.702387	-0.050044	4.815572
238.983913	7999.901439	10.707392	-0.050062	4.815574
238.981788	7999.890745	10.712397	-0.050062	4.815571
239.063175	7999.919845	10.717402	-0.050077	4.815579
239.182027	7999.903643	10.722407	-0.050100	4.815574
238.895733	7999.899008	10.727411	-0.050047	4.815574
239.062780	7999.945515	10.732416	-0.050078	4.815587
238.806590	7999.917880	10.737421	-0.050030	4.815580
239.052007	7999.916547	10.742426	-0.050076	4.815578
238.938317	7999.909378	10.747431	-0.050055	4.815577
238.816981	7999.901017	10.752435	-0.050033	4.815575
239.096038	7999.944007	10.757440	-0.050085	4.815586
238.949419	7999.906407	10.762445	-0.050058	4.815576
239.063065	7999.932828	10.767450	-0.050079	4.815583
239.223203	7999.909823	10.772455	-0.050109	4.815576
239.020115	7999.912946	10.777459	-0.050072	4.815577
238.992504	7999.885822	10.782464	-0.050067	4.815570
239.096611	7999.875786	10.787469	-0.050086	4.815566
238.991315	7999.902921	10.792474	-0.050067	4.815575
239.027849	7999.894990	10.797479	-0.050074	4.815572
239.018363	7999.891650	10.802483	-0.050072	4.815571
239.046993	7999.918825	10.807488	-0.050078	4.815579
238.973332	7999.904833	10.812493	-0.050064	4.815575
239.112752	7999.917793	10.817498	-0.050091	4.815578
239.084157	7999.894924	10.822503	-0.050085	4.815572
238.953915	7999.916314	10.827507	-0.050061	4.815579
239.183531	7999.930740	10.832512	-0.050104	4.815582
239.020725	7999.899283	10.837517	-0.050074	4.815573
238.987883	7999.952152	10.842522	-0.050068	4.815589
239.046856	7999.902945	10.847527	-0.050079	4.815574
238.975837	7999.890064	10.852531	-0.050066	4.815571
239.079446	7999.902442	10.857536	-0.050086	4.815574
239.116400	7999.916940	10.862541	-0.050093	4.815578
239.016617	7999.940960	10.867546	-0.050075	4.815586
239.097940	7999.913471	10.872551	-0.050090	4.815577
239.004979	7999.904504	10.877555	-0.050073	4.815575
238.969094	7999.943443	10.882560	-0.050066	4.815587
239.061214	7999.937483	10.887565	-0.050084	4.815584
239.164793	7999.935981	10.892570	-0.050103	4.815583
239.095780	7999.918861	10.897575	-0.050091	4.815579
239.235159	7999.898721	10.902579	-0.050117	4.815572
239.221676	7999.929483	10.907584	-0.050114	4.815581
239.141690	7999.903643	10.912589	-0.050100	4.815574
239.086442	7999.928388	10.917594	-0.050090	4.815582
239.158749	7999.924241	10.922599	-0.050103	4.815580
238.977617	7999.911706	10.927603	-0.050070	4.815577
239.177077	7999.941657	10.932608	-0.050107	4.815585
239.258599	7999.909900	10.937613	-0.050122	4.815575
239.143558	7999.929402	10.942618	-0.050101	4.815582
239.337168	7999.938972	10.947623	-0.050137	4.815583
239.015543	7999.909205	10.952627	-0.050078	4.815576
239.272168	7999.931544	10.957632	-0.050126	4.815582
239.274125	7999.899562	10.962637	-0.050126	4.815572
239.272951	7999.924117	10.967642	-0.050126	4.815579
239.297659	7999.919198	10.972647	-0.050131	4.815578
239.152978	7999.904051	10.977651	-0.050104	4.815574
239.228332	7999.942663	10.982656	-0.050119	4.815585
239.260622	7999.919715	10.987661	-0.050125	4.815578
239.264923	7999.906990	10.992666	-0.050126	4.815574
239.406349	7999.915712	10.997671	-0.050152	4.815576
239.303939	7999.896981	11.002675	-0.050133	4.815571
239.460836	7999.916632	11.007680	-0.050163	4.815576
239.233351	7999.899072	11.012685	-0.050121	4.815572
239.180131	7999.913172	11.017690	-0.050111	4.815577
239.279141	7999.952169	11.022695	-0.050130	4.815587
239.162959	7999.946027	11.027699	-0.050108	4.815586
239.224002	7999.949171	11.032704	-0.050120	4.815587
239.309377	7999.886513	11.037709	-0.050136	4.815568
239.370847	7999.909952	11.042714	-0.050147	4.815575
239.462152	7999.942417	11.047719	-0.050165	4.815584
239.279676	7999.887150	11.052723	-0.050131	4.815568
239.254187	7999.919852	11.057728	-0.050126	4.815578
239.227287	7999.891672	11.062733	-0.050122	4.815570
239.223003	7999.921516	11.067738	-0.050121	4.815579
239.180587	7999.910166	11.072743	-0.050113	4.815576
239.212327	7999.924580	11.077747	-0.050119	4.815580
239.240329	7999.959219	11.082752	-0.050125	4.815590
239.249236	7999.925214	11.087757	-0.050127	4.815580
239.300807	7999.925002	11.092762	-0.050136	4.815579
239.305254	7999.922956	11.097767	-0.050137	4.815579
239.229965	7999.910005	11.102771	-0.050124	4.815575
239.390092	7999.979891	11.107776	-0.050154	4.815595
239.237867	7999.957147	11.112781	-0.050126	4.815589
239.093822	7999.947349	11.117786	-0.050099	4.815587
239.286950	7999.930219	11.122791	-0.050135	4.815581
239.438424	7999.912411	11.127795	-0.050163	4.815575
239.546749	7999.924867	11.132800	-0.050184	4.815578
239.298695	7999.900565	11.137805	-0.050138	4.815572
239.180230	7999.917876	11.142810	-0.050116	4.815578
239.367998	7999.904929	11.147815	-0.050151	4.815573
239.361375	7999.906974	11.152819	-0.050150	4.815574
239.409544	7999.928061	11.157824	-0.050159	4.815580
239.380990	7999.900922	11.162829	-0.050154	4.815572
239.242484	7999.910433	11.167834	-0.050129	4.815575
239.344574	7999.900364	11.172839	-0.050148	4.815572
239.331188	7999.903367	11.177843	-0.050145	4.815573
239.460976	7999.921510	11.182848	-0.050170	4.815577
239.245537	7999.897739	11.187853	-0.050130	4.815572
239.295039	7999.934863	11.192858	-0.050139	4.815582
239.247791	7999.911690	11.197863	-0.050131	4.815576
239.223949	7999.915591	11.202867	-0.050126	4.815577
239.438992	7999.939390	11.207872	-0.050167	4.815583
239.388777	7999.903356	11.212877	-0.050158	4.815572
239.412539	7999.921911	11.217882	-0.050162	4.815578
239.613476	7999.918788	11.222887	-0.050200	4.815576
239.557427	7999.917894	11.227891	-0.050190	4.815576
239.378571	7999.943833	11.232896	-0.050156	4.815584
239.413817	7999.892105	11.237901	-0.050163	4.815569
239.419207	7999.905022	11.242906	-0.050164	4.815573
239.281581	7999.932698	11.247911	-0.050139	4.815582
239.285170	7999.913555	11.252915	-0.050140	4.815576
239.377242	7999.973793	11.257920	-0.050157	4.815593
239.387848	7999.903514	11.262925	-0.050159	4.815572
239.505091	7999.920385	11.267930	-0.050181	4.815577
239.414174	7999.926398	11.272935	-0.050165	4.815579
239.384834	7999.899246	11.277939	-0.050159	4.815571
239.569014	7999.931085	11.282944	-0.050194	4.815580
239.505453	7999.912986	11.287949	-0.050182	4.815575
239.468449	7999.919875	11.292954	-0.050176	4.815577
239.362955	7999.921381	11.297959	-0.050156	4.815578
239.257098	7999.891917	11.302963	-0.050137	4.815570
239.276593	7999.939231	11.307968	-0.050140	4.815583
239.404700	7999.898622	11.312973	-0.050164	4.815571
239.315406	7999.912136	11.317978	-0.050148	4.815575
239.274832	7999.928577	11.322983	-0.050141	4.815580
239.439727	7999.916326	11.327987	-0.050172	4.815576
239.556266	7999.939592	11.332992	-0.050194	4.815582
239.350479	7999.905301	11.337997	-0.050155	4.815573
239.279980	7999.923391	11.343002	-0.050142	4.815579
239.420883	7999.917157	11.348007	-0.050169	4.815576
239.377498	7999.920740	11.353011	-0.050161	4.815577
239.415948	7999.956617	11.358016	-0.050168	4.815588
239.447186	7999.919772	11.363021	-0.050174	4.815577
239.312823	7999.905860	11.368026	-0.050150	4.815573
239.431608	7999.908876	11.373031	-0.050172	4.815574
239.532998	7999.889187	11.378035	-0.050191	4.815567
239.587671	7999.923192	11.383040	-0.050201	4.815577
239.485048	7999.898051	11.388045	-0.050182	4.815570
239.464155	7999.905203	11.393050	-0.050179	4.815572
239.548984	7999.908734	11.398055	-0.050195	4.815573
239.433797	7999.895135	11.403059	-0.050173	4.815570
239.404372	7999.929908	11.408064	-0.050168	4.815580
239.416917	7999.897030	11.413069	-0.050171	4.815570
239.403909	7999.926732	11.418074	-0.050168	4.815579
239.402327	7999.910708	11.423079	-0.050168	4.815574
239.400452	7999.888273	11.428083	-0.050168	4.815568
239.604732	7999.925777	11.433088	-0.050206	4.815578
239.637643	7999.882553	11.438093	-0.050213	4.815565
239.584356	7999.923345	11.443098	-0.050203	4.815577
239.594727	7999.912854	11.448103	-0.050205	4.815574
239.444429	7999.900819	11.453107	-0.050177	4.815571
239.385621	7999.931912	11.458112	-0.050167	4.815581
239.547477	7999.897189	11.463117	-0.050197	4.815570
239.365440	7999.911331	11.468122	-0.050163	4.815575
239.499954	7999.926348	11.473127	-0.050189	4.815578
239.396773	7999.918281	11.478131	-0.050170	4.815577
239.521598	7999.932073	11.483136	-0.050193	4.815580
239.546949	7999.900470	11.488141	-0.050198	4.815571
239.685221	7999.912345	11.493146	-0.050224	4.815573
239.758318	7999.929566	11.498151	-0.050238	4.815578
239.669826	7999.886504	11.503155	-0.050221	4.815566
239.618630	7999.920924	11.508160	-0.050212	4.815576
239.759401	7999.914688	11.513165	-0.050238	4.815574
239.640716	7999.927724	11.518170	-0.050217	4.815578
239.529312	7999.933404	11.523175	-0.050196	4.815580
239.256574	7999.888415	11.528179	-0.050145	4.815568
239.470412	7999.927142	11.533184	-0.050185	4.815579
239.522870	7999.890642	11.538189	-0.050195	4.815568
239.504738	7999.902110	11.543194	-0.050192	4.815571
239.640487	7999.908604	11.548199	-0.050218	4.815572
239.574229	7999.875513	11.553203	-0.050206	4.815563
239.636563	7999.906440	11.558208	-0.050217	4.815572
239.697958	7999.898913	11.563213	-0.050229	4.815569
239.689512	7999.935096	11.568218	-0.050228	4.815580
239.532904	7999.944312	11.573223	-0.050199	4.815583
239.534997	7999.918738	11.578227	-0.050199	4.815576
239.657311	7999.938895	11.583232	-0.050222	4.815581
239.546293	7999.916821	11.588237	-0.050202	4.815575
239.504229	7999.917222	11.593242	-0.050194	4.815576
239.673854	7999.930674	11.598247	-0.050226	4.815579
239.646969	7999.913171	11.603251	-0.050221	4.815574
239.734595	7999.926357	11.608256	-0.050238	4.815577
239.663793	7999.926291	11.613261	-0.050225	4.815577
239.779722	7999.891890	11.618266	-0.050246	4.815567
239.773271	7999.927038	11.623271	-0.050245	4.815577
239.510072	7999.911032	11.628275	-0.050197	4.815574
239.764792	7999.916257	11.633280	-0.050244	4.815574
239.768404	7999.898182	11.638285	-0.050245	4.815569
239.681996	7999.918149	11.643290	-0.050229	4.815575
239.823838	7999.942895	11.648295	-0.050256	4.815582
239.868627	7999.919082	11.653299	-0.050264	4.815574
239.756547	7999.916210	11.658304	-0.050244	4.815574
239.571358	7999.902539	11.663309	-0.050209	4.815571
239.675753	7999.907457	11.668314	-0.050229	4.815572
239.769542	7999.911134	11.673319	-0.050247	4.815572
239.693576	7999.889630	11.678323	-0.050233	4.815567
239.746895	7999.928952	11.683328	-0.050243	4.815578
239.864418	7999.925541	11.688333	-0.050265	4.815576
239.840329	7999.940115	11.693338	-0.050261	4.815581
239.772502	7999.920878	11.698343	-0.050248	4.815575
239.683905	7999.915184	11.703347	-0.050232	4.815574
239.586862	7999.964875	11.708352	-0.050214	4.815589
239.730417	7999.904230	11.713357	-0.050241	4.815571
239.935427	7999.942815	11.718362	-0.050279	4.815581
239.763198	7999.901594	11.723367	-0.050247	4.815570
239.585479	7999.894451	11.728371	-0.050215	4.815568
239.728391	7999.935230	11.733376	-0.050241	4.815580
239.716517	7999.903022	11.738381	-0.050239	4.815570
239.777893	7999.930731	11.743386	-0.050251	4.815578
239.781715	7999.935081	11.748391	-0.050252	4.815579
239.854412	7999.939483	11.753395	-0.050266	4.815580
239.898667	7999.956236	11.758400	-0.050274	4.815585
239.772657	7999.906157	11.763405	-0.050251	4.815571
239.954033	7999.915529	11.768410	-0.050285	4.815573
240.012284	7999.915426	11.773415	-0.050296	4.815572
239.538788	7999.907745	11.778419	-0.050208	4.815572
239.801083	7999.934449	11.783424	-0.050257	4.815579
239.776473	7999.910576	11.788429	-0.050252	4.815572
239.874286	7999.924996	11.793434	-0.050271	4.815576
240.057358	7999.944006	11.798439	-0.050305	4.815581
239.980871	7999.899003	11.803443	-0.050291	4.815568
240.035544	7999.940483	11.808448	-0.050302	4.815580
239.947640	7999.968968	11.813453	-0.050285	4.815588
239.830709	7999.944661	11.818458	-0.050264	4.815582
239.921295	7999.957896	11.823463	-0.050281	4.815585
239.756311	7999.927470	11.828467	-0.050250	4.815577
239.852600	7999.965356	11.833472	-0.050268	4.815588
240.037060	7999.961966	11.838477	-0.050303	4.815586
239.858638	7999.938795	11.843482	-0.050270	4.815580
240.028065	7999.956516	11.848487	-0.050302	4.815584
239.948509	7999.927478	11.853491	-0.050287	4.815576
240.023927	7999.962889	11.858496	-0.050301	4.815586
239.865190	7999.921887	11.863501	-0.050272	4.815575
239.851471	7999.945171	11.868506	-0.050270	4.815582
239.920219	7999.932426	11.873511	-0.050283	4.815578
239.808053	7999.909265	11.878515	-0.050262	4.815572
239.903462	7999.943933	11.883520	-0.050280	4.815581
239.952997	7999.926604	11.888525	-0.050289	4.815576
239.868876	7999.936999	11.893530	-0.050274	4.815579
239.743944	7999.923240	11.898535	-0.050251	4.815576
239.719428	7999.924994	11.903539	-0.050246	4.815577
239.927252	7999.945474	11.908544	-0.050285	4.815582
239.759096	7999.931012	11.913549	-0.050254	4.815578
239.839374	7999.902438	11.918554	-0.050269	4.815569
239.834345	7999.927999	11.923559	-0.050269	4.815577
239.806974	7999.922233	11.928563	-0.050264	4.815575
239.891980	7999.950325	11.933568	-0.050280	4.815583
239.850125	7999.913359	11.938573	-0.050272	4.815572
239.844045	7999.925023	11.943578	-0.050271	4.815576
239.977780	7999.952840	11.948583	-0.050296	4.815583
240.118828	7999.927390	11.953587	-0.050323	4.815575
240.138402	7999.937335	11.958592	-0.050327	4.815578
240.081428	7999.916139	11.963597	-0.050316	4.815572
240.111099	7999.930519	11.968602	-0.050322	4.815576
239.931430	7999.904125	11.973607	-0.050289	4.815569
239.976261	7999.868568	11.978611	-0.050297	4.815559
239.954436	7999.924820	11.983616	-0.050293	4.815575
239.817498	7999.927950	11.988621	-0.050268	4.815577
239.793364	7999.940387	11.993626	-0.050264	4.815581
239.807586	7999.929959	11.998631	-0.050267	4.815577
239.807789	7999.912896	12.003635	-0.050267	4.815572
239.838698	7999.910212	12.008640	-0.050273	4.815572
239.868477	7999.931000	12.013645	-0.050279	4.815577
239.801911	7999.918190	12.018650	-0.050266	4.815574
240.129773	7999.939554	12.023655	-0.050328	4.815579
239.827982	7999.909039	12.028659	-0.050272	4.815571
239.878262	7999.925890	12.033664	-0.050281	4.815576
239.892394	7999.926137	12.038669	-0.050284	4.815576
240.119559	7999.907425	12.043674	-0.050326	4.815569
240.082008	7999.920713	12.048679	-0.050320	4.815573
240.016479	7999.918597	12.053683	-0.050308	4.815573
239.939016	7999.935506	12.058688	-0.050293	4.815578
240.026447	7999.959367	12.063693	-0.050310	4.815585
239.842658	7999.920093	12.068698	-0.050276	4.815574
240.017493	7999.964595	12.073703	-0.050309	4.815587
239.719242	7999.933070	12.078707	-0.050253	4.815579
239.991207	7999.928967	12.083712	-0.050304	4.815576
240.097174	7999.926436	12.088717	-0.050324	4.815575
240.040526	7999.909516	12.093722	-0.050314	4.815570
239.766253	7999.913616	12.098727	-0.050263	4.815573
239.852625	7999.880870	12.103731	-0.050279	4.815563
239.867782	7999.939859	12.108736	-0.050282	4.815580
239.997352	7999.915290	12.113741	-0.050306	4.815572
240.011282	7999.913398	12.118746	-0.050309	4.815572
240.151975	7999.929584	12.123751	-0.050336	4.815576
240.090095	7999.925391	12.128755	-0.050324	4.815575
240.050175	7999.941843	12.133760	-0.050317	4.815580
240.089382	7999.941430	12.138765	-0.050325	4.815579
240.247244	7999.917321	12.143770	-0.050354	4.815572
240.228567	7999.927712	12.148775	-0.050351	4.815575
239.965184	7999.911702	12.153779	-0.050302	4.815571
240.072813	7999.943366	12.158784	-0.050322	4.815580
240.077158	7999.910354	12.163789	-0.050323	4.815570
239.734961	7999.912281	12.168794	-0.050260	4.815572
239.872188	7999.930546	12.173799	-0.050286	4.815577
239.756376	7999.893445	12.178803	-0.050264	4.815567
240.048187	7999.930239	12.183808	-0.050319	4.815576
240.369159	7999.944017	12.188813	-0.050379	4.815579
240.203379	7999.931729	12.193818	-0.050348	4.815576
240.112727	7999.944153	12.198823	-0.050331	4.815580
239.999116	7999.907087	12.203827	-0.050310	4.815570
239.895800	7999.937457	12.208832	-0.050291	4.815579
239.876014	7999.912595	12.213837	-0.050288	4.815572
239.900045	7999.906596	12.218842	-0.050292	4.815570
239.927721	7999.922012	12.223847	-0.050298	4.815574
240.008524	7999.900920	12.228851	-0.050313	4.815568
239.745478	7999.915880	12.233856	-0.050264	4.815573
240.009027	7999.906302	12.238861	-0.050314	4.815569
240.097999	7999.908833	12.243866	-0.050330	4.815570
239.990080	7999.944467	12.248871	-0.050310	4.815581
239.697923	7999.938666	12.253875	-0.050256	4.815580
239.919328	7999.933741	12.258880	-0.050298	4.815578
240.041653	7999.928273	12.263885	-0.050321	4.815576
240.010221	7999.914967	12.268890	-0.050315	4.815572
240.020378	7999.935436	12.273895	-0.050317	4.815578
239.987053	7999.909286	12.278899	-0.050311	4.815570
239.987581	7999.933870	12.283904	-0.050311	4.815577
240.076872	7999.905442	12.288909	-0.050328	4.815569
240.156391	7999.906752	12.293914	-0.050343	4.815569
240.201873	7999.932067	12.298919	-0.050352	4.815576
240.008129	7999.900105	12.303923	-0.050316	4.815567
240.093917	7999.914330	12.308928	-0.050332	4.815571
240.237069	7999.909201	12.313933	-0.050359	4.815569
240.076969	7999.905547	12.318938	-0.050329	4.815569
239.956536	7999.931367	12.323943	-0.050307	4.815577
240.000528	7999.925694	12.328947	-0.050316	4.815575
240.069704	7999.948190	12.333952	-0.050329	4.815581
239.983895	7999.946812	12.338957	-0.050313	4.815581
239.871627	7999.907634	12.343962	-0.050292	4.815570
240.011871	7999.932354	12.348967	-0.050318	4.815577
239.860966	7999.906427	12.353971	-0.050291	4.815570
240.025932	7999.926210	12.358976	-0.050321	4.815575
240.041797	7999.925418	12.363981	-0.050325	4.815575
239.983820	7999.921289	12.368986	-0.050314	4.815574
240.220704	7999.962529	12.373991	-0.050358	4.815585
240.148820	7999.919736	12.378995	-0.050345	4.815572
240.111809	7999.921287	12.384000	-0.050338	4.815573
240.259440	7999.908756	12.389005	-0.050366	4.815569
240.093008	7999.917812	12.394010	-0.050335	4.815572
240.302250	7999.929774	12.399015	-0.050375	4.815575
240.121459	7999.902293	12.404019	-0.050341	4.815567
240.106228	7999.945840	12.409024	-0.050338	4.815580
240.029386	7999.927524	12.414029	-0.050324	4.815575
239.895371	7999.941378	12.419034	-0.050300	4.815580
240.115807	7999.951387	12.424039	-0.050341	4.815582
240.130100	7999.913198	12.429043	-0.050344	4.815571
239.908554	7999.935238	12.434048	-0.050303	4.815578
239.984698	7999.935426	12.439053	-0.050317	4.815578
239.978658	7999.912922	12.444058	-0.050316	4.815571
240.199644	7999.967785	12.449063	-0.050357	4.815586
240.193069	7999.918579	12.454067	-0.050356	4.815572
240.076894	7999.917775	12.459072	-0.050335	4.815572
240.197038	7999.921881	12.464077	-0.050358	4.815573
240.189217	7999.921771	12.469082	-0.050356	4.815573
240.211373	7999.957384	12.474087	-0.050361	4.815583
240.241219	7999.936532	12.479091	-0.050366	4.815577
240.065584	7999.917677	12.484096	-0.050334	4.815572
239.981452	7999.923801	12.489101	-0.050318	4.815574
239.963987	7999.894705	12.494106	-0.050315	4.815566
240.195564	7999.910233	12.499111	-0.050359	4.815569
240.188368	7999.888778	12.504115	-0.050357	4.815563
240.162273	7999.930013	12.509120	-0.050353	4.815575
240.139789	7999.935004	12.514125	-0.050349	4.815577
240.028768	7999.936419	12.519130	-0.050328	4.815578
240.149951	7999.957626	12.524135	-0.050351	4.815583
240.087626	7999.901107	12.529139	-0.050340	4.815567
240.206175	7999.934017	12.534144	-0.050362	4.815576
240.131930	7999.937098	12.539149	-0.050348	4.815577
240.315881	7999.936903	12.544154	-0.050383	4.815577
240.199298	7999.932889	12.549159	-0.050361	4.815576
239.952757	7999.933168	12.554163	-0.050316	4.815577
239.966754	7999.934481	12.559168	-0.050318	4.815577
240.049866	7999.927308	12.564173	-0.050334	4.815575
240.044975	7999.913365	12.569178	-0.050333	4.815571
239.841801	7999.933569	12.574183	-0.050296	4.815578
239.961921	7999.884288	12.579187	-0.050318	4.815563
240.176770	7999.926237	12.584192	-0.050358	4.815574
240.236129	7999.909068	12.589197	-0.050370	4.815569
240.236264	7999.911223	12.594202	-0.050370	4.815569
240.148266	7999.943977	12.599207	-0.050354	4.815579
240.131957	7999.936255	12.604211	-0.050351	4.815577
240.106981	7999.957221	12.609216	-0.050346	4.815583
240.275147	7999.968515	12.614221	-0.050378	4.815586
240.231747	7999.938997	12.619226	-0.050370	4.815577
240.137072	7999.963101	12.624231	-0.050353	4.815585
240.189926	7999.910590	12.629235	-0.050363	4.815569
240.223957	7999.921838	12.634240	-0.050369	4.815572
240.208288	7999.910923	12.639245	-0.050367	4.815569
240.242120	7999.918965	12.644250	-0.050373	4.815572
240.424990	7999.935837	12.649255	-0.050407	4.815576
240.426132	7999.927331	12.654259	-0.050408	4.815573
240.090049	7999.926154	12.659264	-0.050345	4.815574
240.112632	7999.967112	12.664269	-0.050350	4.815586
239.979654	7999.924393	12.669274	-0.050325	4.815574
240.171165	7999.957421	12.674279	-0.050361	4.815583
240.200999	7999.917349	12.679283	-0.050367	4.815571
240.229016	7999.932771	12.684288	-0.050372	4.815576
240.302315	7999.899812	12.689293	-0.050386	4.815566
240.047626	7999.907433	12.694298	-0.050339	4.815569
240.355728	7999.945561	12.699303	-0.050396	4.815579
240.197133	7999.946202	12.704307	-0.050367	4.815580
240.181711	7999.939562	12.709312	-0.050364	4.815578
240.386601	7999.945047	12.714317	-0.050403	4.815578
240.303861	7999.942651	12.719322	-0.050387	4.815578
240.478535	7999.943373	12.724327	-0.050420	4.815577
240.282119	7999.926316	12.729331	-0.050384	4.815573
240.223469	7999.942463	12.734336	-0.050373	4.815578
240.282910	7999.924228	12.739341	-0.050384	4.815573
240.220513	7999.902943	12.744346	-0.050373	4.815567
240.394024	7999.951695	12.749351	-0.050405	4.815580
240.408571	7999.923120	12.754355	-0.050408	4.815572
240.356825	7999.927634	12.759360	-0.050399	4.815573
240.420637	7999.903063	12.764365	-0.050411	4.815566
240.476310	7999.906121	12.769370	-0.050422	4.815567
240.391295	7999.932518	12.774375	-0.050406	4.815575
240.284940	7999.910518	12.779379	-0.050386	4.815569
240.320011	7999.916444	12.784384	-0.050393	4.815570
240.357518	7999.929885	12.789389	-0.050400	4.815574
240.479192	7999.938287	12.794394	-0.050423	4.815576
240.640348	7999.938790	12.799399	-0.050453	4.815575
240.495600	7999.912963	12.804403	-0.050427	4.815568
240.422751	7999.936353	12.809408	-0.050413	4.815576
240.380346	7999.936749	12.814413	-0.050405	4.815576
240.355897	7999.911810	12.819418	-0.050401	4.815569
240.389490	7999.920916	12.824423	-0.050408	4.815571
240.255659	7999.919824	12.829427	-0.050383	4.815572
240.424341	7999.948211	12.834432	-0.050414	4.815579
240.345987	7999.950157	12.839437	-0.050400	4.815580
240.277307	7999.935177	12.844442	-0.050387	4.815576
240.265118	7999.925386	12.849447	-0.050385	4.815573
240.369218	7999.917486	12.854451	-0.050405	4.815570
240.431754	7999.950553	12.859456	-0.050417	4.815580
240.368456	7999.947406	12.864461	-0.050405	4.815579
240.245803	7999.926209	12.869466	-0.050383	4.815573
240.479928	7999.932169	12.874471	-0.050426	4.815574
240.200861	7999.906293	12.879475	-0.050375	4.815568
240.294460	7999.949475	12.884480	-0.050392	4.815580
240.341371	7999.918222	12.889485	-0.050401	4.815571
240.271505	7999.935255	12.894490	-0.050388	4.815576
240.402782	7999.917120	12.899495	-0.050413	4.815570
240.311640	7999.890029	12.904499	-0.050396	4.815562
240.232747	7999.926135	12.909504	-0.050382	4.815573
240.328965	7999.931988	12.914509	-0.050400	4.815575
240.257991	7999.936189	12.919514	-0.050387	4.815576
240.371521	7999.943392	12.924519	-0.050408	4.815578
240.286711	7999.896117	12.929523	-0.050393	4.815564
240.447011	7999.931841	12.934528	-0.050423	4.815574
240.522949	7999.960855	12.939533	-0.050437	4.815582
240.440085	7999.926424	12.944538	-0.050422	4.815572
240.417335	7999.947426	12.949543	-0.050418	4.815579
240.418466	7999.949598	12.954547	-0.050418	4.815579
240.351890	7999.954939	12.959552	-0.050406	4.815581
240.563134	7999.941308	12.964557	-0.050445	4.815576
240.386590	7999.912827	12.969562	-0.050413	4.815569
240.343527	7999.936703	12.974567	-0.050405	4.815576
240.401337	7999.928050	12.979571	-0.050416	4.815573
240.293223	7999.966884	12.984576	-0.050396	4.815585
240.559264	7999.941331	12.989581	-0.050446	4.815576
240.399535	7999.921666	12.994586	-0.050416	4.815571
240.470750	7999.937790	12.999591	-0.050430	4.815576
240.419618	7999.894266	13.004595	-0.050420	4.815563
240.378834	7999.910704	13.009600	-0.050413	4.815568
240.441591	7999.910674	13.014605	-0.050425	4.815568
240.562733	7999.906255	13.019610	-0.050448	4.815566
240.638768	7999.922458	13.024615	-0.050462	4.815570
240.509431	7999.924642	13.029619	-0.050438	4.815572
240.454254	7999.921627	13.034624	-0.050428	4.815571
240.711699	7999.941848	13.039629	-0.050476	4.815576
240.423324	7999.903006	13.044634	-0.050423	4.815566
240.613578	7999.936015	13.049639	-0.050458	4.815574
240.620760	7999.908388	13.054643	-0.050460	4.815566
240.560684	7999.957612	13.059648	-0.050449	4.815581
240.592405	7999.947468	13.064653	-0.050455	4.815578
240.524994	7999.929305	13.069658	-0.050443	4.815573
240.660747	7999.949682	13.074663	-0.050468	4.815578
240.460053	7999.904793	13.079667	-0.050431	4.815566
240.431099	7999.924626	13.084672	-0.050426	4.815572
240.582132	7999.935642	13.089677	-0.050454	4.815574
240.522063	7999.922937	13.094682	-0.050443	4.815571
240.588956	7999.953939	13.099687	-0.050456	4.815580
240.766818	7999.926952	13.104691	-0.050489	4.815571
240.781175	7999.952830	13.109696	-0.050492	4.815578
240.680190	7999.945865	13.114701	-0.050473	4.815577
240.554053	7999.932086	13.119706	-0.050450	4.815573
240.611784	7999.953329	13.124711	-0.050461	4.815579
240.511350	7999.946374	13.129715	-0.050442	4.815578
240.621557	7999.952455	13.134720	-0.050463	4.815579
240.650827	7999.976439	13.139725	-0.050469	4.815586
240.547458	7999.924590	13.144730	-0.050450	4.815571
240.852308	7999.948786	13.149735	-0.050507	4.815577
240.720198	7999.927435	13.154739	-0.050482	4.815571
240.826880	7999.952678	13.159744	-0.050502	4.815578
240.731898	7999.944744	13.164749	-0.050485	4.815576
240.563696	7999.928144	13.169754	-0.050454	4.815572
240.466626	7999.932989	13.174759	-0.050436	4.815574
240.580007	7999.930580	13.179763	-0.050457	4.815573
240.423841	7999.933396	13.184768	-0.050428	4.815574
240.527166	7999.937229	13.189773	-0.050448	4.815575
240.518102	7999.932828	13.194778	-0.050446	4.815574
240.580264	7999.968024	13.199783	-0.050458	4.815584
240.446979	7999.908215	13.204787	-0.050433	4.815567
240.632820	7999.936881	13.209792	-0.050468	4.815574
240.615464	7999.929142	13.214797	-0.050465	4.815572
240.458792	7999.941559	13.219802	-0.050436	4.815577
240.664487	7999.956668	13.224807	-0.050475	4.815580
240.522021	7999.944758	13.229811	-0.050448	4.815577
240.362772	7999.937914	13.234816	-0.050419	4.815576
240.586261	7999.943702	13.239821	-0.050461	4.815577
240.473316	7999.925866	13.244826	-0.050440	4.815572
240.602737	7999.936530	13.249831	-0.050464	4.815574
240.581233	7999.930859	13.254835	-0.050460	4.815573
240.497505	7999.933785	13.259840	-0.050445	4.815574
240.510021	7999.954293	13.264845	-0.050447	4.815580
240.345520	7999.920670	13.269850	-0.050417	4.815571
240.568837	7999.938200	13.274855	-0.050459	4.815575
240.458680	7999.917206	13.279859	-0.050438	4.815569
240.328816	7999.935399	13.284864	-0.050414	4.815575
240.704715	7999.967157	13.289869	-0.050485	4.815583
240.742267	7999.930413	13.294874	-0.050492	4.815572
240.758599	7999.930696	13.299879	-0.050495	4.815572
240.694212	7999.939276	13.304883	-0.050483	4.815575
240.661362	7999.927013	13.309888	-0.050477	4.815571
240.745237	7999.963631	13.314893	-0.050493	4.815582
240.319951	7999.917224	13.319898	-0.050414	4.815570
240.597361	7999.936702	13.324903	-0.050466	4.815574
240.449342	7999.917227	13.329907	-0.050439	4.815569
240.328474	7999.917414	13.334912	-0.050416	4.815570
240.548016	7999.928477	13.339917	-0.050457	4.815572
240.603026	7999.926185	13.344922	-0.050468	4.815571
240.626413	7999.954345	13.349927	-0.050472	4.815579
240.476250	7999.896396	13.354931	-0.050445	4.815563
240.620041	7999.925446	13.359936	-0.050472	4.815571
240.562895	7999.923466	13.364941	-0.050461	4.815571
240.618048	7999.895551	13.369946	-0.050472	4.815562
240.810494	7999.938206	13.374951	-0.050508	4.815574
240.831235	7999.914002	13.379955	-0.050512	4.815567
240.746032	7999.926514	13.384960	-0.050496	4.815571
240.831390	7999.936462	13.389965	-0.050512	4.815573
240.763155	7999.921488	13.394970	-0.050500	4.815569
240.801827	7999.984065	13.399975	-0.050507	4.815587
240.585916	7999.937860	13.404979	-0.050467	4.815575
240.671839	7999.936071	13.409984	-0.050483	4.815574
240.605333	7999.943549	13.414989	-0.050471	4.815576
240.501542	7999.930133	13.419994	-0.050452	4.815573
240.664843	7999.946687	13.424999	-0.050483	4.815577
240.755282	7999.919346	13.430003	-0.050500	4.815568
240.546808	7999.919175	13.435008	-0.050461	4.815569
240.584432	7999.951837	13.440013	-0.050468	4.815579
240.520920	7999.919857	13.445018	-0.050457	4.815570
240.693460	7999.931222	13.450023	-0.050489	4.815572
240.574026	7999.896196	13.455027	-0.050467	4.815562
240.709838	7999.936862	13.460032	-0.050492	4.815574
240.836463	7999.945346	13.465037	-0.050516	4.815576
240.616848	7999.932181	13.470042	-0.050475	4.815573
240.655463	7999.943504	13.475047	-0.050483	4.815576
240.806631	7999.960929	13.480051	-0.050511	4.815580
240.595309	7999.928679	13.485056	-0.050472	4.815572
240.693024	7999.963386	13.490061	-0.050490	4.815582
240.567239	7999.923986	13.495066	-0.050467	4.815571
240.861782	7999.966166	13.500071	-0.050522	4.815582
240.566810	7999.970995	13.505075	-0.050468	4.815584
240.632707	7999.972084	13.510080	-0.050480	4.815584
240.730844	7999.938462	13.515085	-0.050498	4.815574
240.643202	7999.922105	13.520090	-0.050482	4.815570
240.823594	7999.958157	13.525095	-0.050516	4.815579
240.776051	7999.922165	13.530099	-0.050507	4.815569
240.715518	7999.937214	13.535104	-0.050496	4.815574
240.725627	7999.941667	13.540109	-0.050498	4.815575
240.892786	7999.911302	13.545114	-0.050530	4.815565
240.866133	7999.947190	13.550119	-0.050525	4.815576
240.753779	7999.925092	13.555123	-0.050504	4.815570
240.684209	7999.939994	13.560128	-0.050492	4.815575
240.802574	7999.913107	13.565133	-0.050514	4.815566
240.704093	7999.924336	13.570138	-0.050496	4.815570
240.622570	7999.948653	13.575143	-0.050481	4.815577
240.666315	7999.916281	13.580147	-0.050489	4.815568
240.722927	7999.927897	13.585152	-0.050500	4.815571
240.915190	7999.948126	13.590157	-0.050536	4.815576
240.743534	7999.907979	13.595162	-0.050504	4.815565
240.580621	7999.959803	13.600167	-0.050474	4.815581
240.485643	7999.928378	13.605171	-0.050456	4.815572
240.506447	7999.923395	13.610176	-0.050460	4.815571
240.718931	7999.952494	13.615181	-0.050500	4.815578
240.720458	7999.923707	13.620186	-0.050501	4.815570
240.773380	7999.926721	13.625191	-0.050511	4.815570
240.652007	7999.914086	13.630195	-0.050488	4.815567
240.745901	7999.940189	13.635200	-0.050506	4.815574
240.744195	7999.951924	13.640205	-0.050506	4.815578
240.714874	7999.919431	13.645210	-0.050501	4.815568
240.860555	7999.939971	13.650215	-0.050528	4.815574
240.928963	7999.919745	13.655219	-0.050541	4.815567
240.808432	7999.928479	13.660224	-0.050519	4.815571
240.967156	7999.935350	13.665229	-0.050548	4.815572
240.712003	7999.925878	13.670234	-0.050501	4.815570
240.549932	7999.946749	13.675239	-0.050471	4.815577
240.760821	7999.929910	13.680243	-0.050511	4.815571
240.649795	7999.917443	13.685248	-0.050490	4.815568
240.733989	7999.960473	13.690253	-0.050506	4.815580
240.630033	7999.941715	13.695258	-0.050487	4.815575
240.871861	7999.962750	13.700263	-0.050532	4.815580
240.849567	7999.913288	13.705267	-0.050528	4.815566
240.753100	7999.925617	13.710272	-0.050510	4.815570
240.814491	7999.934107	13.715277	-0.050522	4.815572
240.686778	7999.898946	13.720282	-0.050498	4.815562
240.926275	7999.942367	13.725287	-0.050543	4.815574
240.966626	7999.921685	13.730291	-0.050551	4.815568
240.901711	7999.931324	13.735296	-0.050539	4.815571
240.784432	7999.953992	13.740301	-0.050517	4.815578
240.850385	7999.916642	13.745306	-0.050530	4.815567
240.737560	7999.931909	13.750311	-0.050509	4.815572
240.843728	7999.916569	13.755315	-0.050529	4.815567
240.841940	7999.929370	13.760320	-0.050529	4.815571
240.880787	7999.964188	13.765325	-0.050536	4.815581
240.686205	7999.924736	13.770330	-0.050500	4.815570
240.758071	7999.941939	13.775335	-0.050514	4.815575
240.771391	7999.934698	13.780339	-0.050516	4.815572
240.633600	7999.919661	13.785344	-0.050491	4.815569
240.625746	7999.951583	13.790349	-0.050490	4.815578
240.597555	7999.925516	13.795354	-0.050485	4.815571
240.885275	7999.955840	13.800359	-0.050538	4.815578
241.006713	7999.941816	13.805363	-0.050561	4.815573
240.562019	7999.923922	13.810368	-0.050479	4.815570
240.753724	7999.968700	13.815373	-0.050515	4.815582
240.764316	7999.917637	13.820378	-0.050517	4.815567
240.753441	7999.951646	13.825383	-0.050515	4.815577
240.601201	7999.948119	13.830387	-0.050487	4.815577
240.641945	7999.927444	13.835392	-0.050495	4.815571
240.864877	7999.935359	13.840397	-0.050536	4.815572
240.787429	7999.925574	13.845402	-0.050522	4.815570
240.825063	7999.962507	13.850407	-0.050529	4.815580
240.597402	7999.927856	13.855411	-0.050487	4.815571
240.637981	7999.916788	13.860416	-0.050495	4.815568
240.754199	7999.919764	13.865421	-0.050517	4.815568
240.705447	7999.922191	13.870426	-0.050508	4.815569
240.708711	7999.951091	13.875431	-0.050509	4.815577
240.714078	7999.962941	13.880435	-0.050510	4.815581
240.625526	7999.951908	13.885440	-0.050493	4.815578
240.661518	7999.949307	13.890445	-0.050500	4.815577
240.544025	7999.928194	13.895450	-0.050479	4.815572
240.722288	7999.943924	13.900455	-0.050512	4.815575
240.732790	7999.940909	13.905459	-0.050514	4.815574
240.631484	7999.921126	13.910464	-0.050496	4.815569
240.902745	7999.945844	13.915469	-0.050546	4.815575
240.752563	7999.930605	13.920474	-0.050518	4.815571
240.690066	7999.953096	13.925479	-0.050507	4.815578
240.636512	7999.920209	13.930483	-0.050497	4.815569
240.693805	7999.916888	13.935488	-0.050508	4.815567
240.847630	7999.961050	13.940493	-0.050537	4.815580
240.680851	7999.919915	13.945498	-0.050506	4.815568
240.662371	7999.933512	13.950503	-0.050503	4.815572
240.835402	7999.932073	13.955507	-0.050535	4.815571
240.628642	7999.906304	13.960512	-0.050497	4.815565
240.789503	7999.946310	13.965517	-0.050527	4.815576
240.914672	7999.936618	13.970522	-0.050551	4.815572
240.908176	7999.969630	13.975527	-0.050550	4.815582
240.679946	7999.925360	13.980531	-0.050507	4.815570
240.592677	7999.929296	13.985536	-0.050491	4.815572
240.715594	7999.949465	13.990541	-0.050514	4.815577
240.489463	7999.904161	13.995546	-0.050472	4.815565
240.487544	7999.939383	14.000551	-0.050472	4.815575
240.704365	7999.919437	14.005555	-0.050513	4.815568
240.531874	7999.938003	14.010560	-0.050481	4.815574
240.669004	7999.969081	14.015565	-0.050507	4.815583
240.819996	7999.917098	14.020570	-0.050535	4.815567
240.662063	7999.945512	14.025575	-0.050506	4.815576
240.795866	7999.954112	14.030579	-0.050531	4.815578
240.713837	7999.928237	14.035584	-0.050516	4.815571
240.779465	7999.946406	14.040589	-0.050528	4.815576
240.611124	7999.916990	14.045594	-0.050497	4.815568
240.636955	7999.965477	14.050599	-0.050502	4.815582
240.736223	7999.960703	14.055603	-0.050521	4.815580
240.575716	7999.953838	14.060608	-0.050491	4.815579
240.639472	7999.960231	14.065613	-0.050503	4.815580
240.663675	7999.949965	14.070618	-0.050508	4.815577
240.619504	7999.975957	14.075623	-0.050500	4.815585
240.537026	7999.936194	14.080627	-0.050485	4.815574
240.615987	7999.924682	14.085632	-0.050500	4.815570
240.574548	7999.971007	14.090637	-0.050492	4.815584
240.615326	7999.933248	14.095642	-0.050500	4.815572
240.644087	7999.938004	14.100647	-0.050505	4.815574
240.577821	7999.929469	14.105651	-0.050493	4.815572
240.737286	7999.934216	14.110656	-0.050523	4.815572
240.758962	7999.949535	14.115661	-0.050527	4.815577
240.682056	7999.911997	14.120666	-0.050513	4.815566
240.821290	7999.940973	14.125671	-0.050539	4.815574
240.665498	7999.904288	14.130675	-0.050511	4.815564
240.650566	7999.914740	14.135680	-0.050508	4.815567
240.827657	7999.928316	14.140685	-0.050541	4.815570
240.812337	7999.892847	14.145690	-0.050539	4.815560
240.754809	7999.939978	14.150695	-0.050528	4.815574
240.817473	7999.906846	14.155699	-0.050540	4.815564
240.660259	7999.917119	14.160704	-0.050511	4.815567
240.982993	7999.943742	14.165709	-0.050571	4.815574
240.937048	7999.907776	14.170714	-0.050563	4.815563
240.981101	7999.959763	14.175719	-0.050571	4.815578
240.796766	7999.941832	14.180723	-0.050537	4.815574
240.693435	7999.924152	14.185728	-0.050518	4.815569
240.832829	7999.937115	14.190733	-0.050544	4.815572
240.681752	7999.900506	14.195738	-0.050516	4.815562
241.077344	7999.934721	14.200743	-0.050590	4.815571
241.048397	7999.937470	14.205747	-0.050585	4.815572
241.073663	7999.937899	14.210752	-0.050590	4.815572
241.091230	7999.967032	14.215757	-0.050593	4.815580
240.971852	7999.938412	14.220762	-0.050571	4.815572
240.831190	7999.950022	14.225767	-0.050545	4.815576
240.947337	7999.913489	14.230771	-0.050567	4.815565
240.711917	7999.924625	14.235776	-0.050523	4.815569
240.980406	7999.963179	14.240781	-0.050574	4.815579
240.700168	7999.942621	14.245786	-0.050522	4.815575
240.776869	7999.955631	14.250791	-0.050536	4.815578
240.988099	7999.938798	14.255795	-0.050576	4.815572
240.765034	7999.302011	14.260800	-0.050534	4.815387

240.736824	7996.017572	14.265805	-0.050527	4.814427
240.786369	7990.570703	14.270810	-0.050533	4.812833
240.828708	7983.926467	14.275815	-0.050536	4.810889
240.833106	7976.625355	14.280819	-0.050533	4.808752
240.634537	7968.997154	14.285824	-0.050491	4.806518
240.966254	7961.210269	14.290829	-0.050548	4.804235
240.762163	7953.400756	14.295834	-0.050505	4.801947
240.574952	7945.356917	14.300839	-0.050465	4.799588
240.741856	7937.442534	14.305843	-0.050491	4.797265
240.585895	7929.362435	14.310848	-0.050457	4.794894
240.473647	7921.443238	14.315853	-0.050431	4.792568
240.373054	7913.397460	14.320858	-0.050407	4.790204
240.418175	7905.382154	14.325863	-0.050411	4.787848
240.506776	7897.361836	14.330867	-0.050422	4.785488
240.075016	7889.404129	14.335872	-0.050337	4.783148
240.408623	7881.421523	14.340877	-0.050394	4.780796
240.440609	7873.431328	14.345882	-0.050395	4.778442
240.301071	7865.404710	14.350887	-0.050364	4.776077
240.405278	7857.431826	14.355891	-0.050378	4.773725
240.456923	7849.348978	14.360896	-0.050383	4.771340
240.255800	7841.387560	14.365901	-0.050340	4.768991
240.063678	7833.414408	14.370906	-0.050300	4.766637
240.260136	7825.334814	14.375911	-0.050331	4.764249
240.233138	7817.475111	14.380915	-0.050321	4.761926
240.158057	7809.341157	14.385920	-0.050302	4.759520
240.144764	7801.435671	14.390925	-0.050295	4.757181
240.025603	7793.335750	14.395930	-0.050267	4.754783
239.990914	7785.323094	14.400935	-0.050256	4.752410
239.947783	7777.319636	14.405939	-0.050243	4.750038
239.933170	7769.304715	14.410944	-0.050235	4.747661
239.769817	7761.353283	14.415949	-0.050200	4.745303
239.798838	7753.379463	14.420954	-0.050200	4.742936
239.728734	7745.372882	14.425959	-0.050182	4.740559
239.967221	7737.373412	14.430963	-0.050221	4.738181
239.637605	7729.289401	14.435968	-0.050155	4.735779
239.580234	7721.327662	14.440973	-0.050139	4.733412
239.616832	7713.337248	14.445978	-0.050141	4.731034
239.588474	7705.282104	14.450983	-0.050131	4.728636
239.527864	7697.317751	14.455987	-0.050114	4.726264
239.339422	7689.266237	14.460992	-0.050074	4.723865
239.447705	7681.318786	14.465997	-0.050089	4.721495
239.420908	7673.289413	14.471002	-0.050079	4.719100
239.437164	7665.332461	14.476007	-0.050077	4.716725
239.440980	7657.291621	14.481011	-0.050073	4.714324
239.307113	7649.291421	14.486016	-0.050043	4.711934
239.193549	7641.276698	14.491021	-0.050017	4.709538
239.260741	7633.317536	14.496026	-0.050025	4.707158
239.209983	7625.285388	14.501031	-0.050010	4.704754
239.094647	7617.342408	14.506035	-0.049984	4.702377
239.089558	7609.256282	14.511040	-0.049978	4.699955
239.295249	7601.345493	14.516045	-0.050011	4.697584
239.131960	7593.300930	14.521050	-0.049975	4.695172
239.119334	7585.302087	14.526055	-0.049968	4.692772
239.119694	7577.298068	14.531059	-0.049963	4.690370
238.895286	7569.260466	14.536064	-0.049916	4.687957
238.806613	7561.267340	14.541069	-0.049895	4.685555
239.024739	7553.276914	14.546074	-0.049930	4.683153
238.928979	7545.295086	14.551079	-0.049908	4.680752
238.708985	7537.320917	14.556083	-0.049862	4.678353
238.684451	7529.281390	14.561088	-0.049852	4.675932
238.720680	7521.239075	14.566093	-0.049854	4.673510
238.624821	7513.113343	14.571098	-0.049831	4.671061
238.344024	7505.198133	14.576103	-0.049774	4.668674
238.514387	7497.253762	14.581107	-0.049800	4.666277
238.468044	7489.157472	14.586112	-0.049787	4.663833
238.285022	7481.271632	14.591117	-0.049748	4.661452
238.298352	7473.244951	14.596122	-0.049745	4.659026
238.336429	7465.265895	14.601127	-0.049747	4.656614
238.314093	7457.249504	14.606131	-0.049738	4.654189
238.122730	7449.201748	14.611136	-0.049697	4.651754
238.225155	7441.206509	14.616141	-0.049711	4.649333
238.063566	7433.237394	14.621146	-0.049676	4.646918
237.996075	7425.202695	14.626151	-0.049659	4.644483
238.260600	7417.271760	14.631155	-0.049703	4.642077
238.033215	7409.216327	14.636160	-0.049655	4.639633
237.904965	7401.310366	14.641165	-0.049627	4.637233
237.958439	7393.206423	14.646170	-0.049632	4.634771
237.996972	7385.157074	14.651175	-0.049634	4.632325
237.784175	7377.192757	14.656179	-0.049589	4.629903
237.594064	7369.169116	14.661184	-0.049549	4.627462
237.766333	7361.218780	14.666189	-0.049576	4.625042
237.609289	7353.231353	14.671194	-0.049541	4.622609
237.612296	7345.167350	14.676199	-0.049537	4.620152
237.635273	7337.228447	14.681203	-0.049536	4.617731
237.444498	7329.192405	14.686208	-0.049496	4.615280
237.644061	7321.168832	14.691213	-0.049528	4.612831
237.694255	7313.148482	14.696218	-0.049532	4.610382
237.811474	7305.162992	14.701223	-0.049549	4.607942
237.559652	7297.165632	14.706227	-0.049497	4.605497
237.480569	7289.157156	14.711232	-0.049477	4.603048
237.598715	7281.198654	14.716237	-0.049494	4.600612
237.253015	7273.204168	14.721242	-0.049425	4.598164
237.288322	7265.170713	14.726247	-0.049426	4.595703
237.463412	7257.155573	14.731251	-0.049454	4.593247
237.375517	7249.074939	14.736256	-0.049433	4.590768
237.218705	7241.110744	14.741261	-0.049398	4.588324
237.210233	7233.107823	14.746266	-0.049392	4.585867
237.187518	7225.117366	14.751271	-0.049383	4.583413
236.962147	7217.182526	14.756275	-0.049336	4.580974
236.972722	7209.134606	14.761280	-0.049333	4.578499
237.201910	7201.179641	14.766285	-0.049370	4.576052
237.153933	7193.116199	14.771290	-0.049356	4.573569
237.011958	7185.112205	14.776295	-0.049325	4.571104
236.983636	7177.129396	14.781299	-0.049315	4.568644
236.963303	7169.124557	14.786304	-0.049306	4.566176
236.979519	7161.134032	14.791309	-0.049304	4.563710
236.688164	7153.144070	14.796314	-0.049244	4.561244
236.685798	7145.148179	14.801319	-0.049239	4.558774
236.656426	7137.203216	14.806323	-0.049229	4.556319
236.556588	7129.121565	14.811328	-0.049205	4.553820
236.953745	7121.118589	14.816333	-0.049274	4.551345
236.819296	7113.097372	14.821338	-0.049244	4.548862
236.696614	7105.112783	14.826343	-0.049216	4.546389
236.814709	7097.109089	14.831347	-0.049233	4.543910
236.610071	7089.111591	14.836352	-0.049190	4.541430
236.525264	7081.128901	14.841357	-0.049169	4.538953
236.615504	7073.149530	14.846362	-0.049181	4.536477
236.660217	7065.108443	14.851367	-0.049184	4.533980
236.472401	7057.117499	14.856371	-0.049144	4.531497
236.332797	7049.072461	14.861376	-0.049113	4.528995
236.405563	7041.122770	14.866381	-0.049122	4.526523
236.273338	7033.072561	14.871386	-0.049092	4.524017
236.343578	7025.118603	14.876391	-0.049100	4.521540
236.375689	7017.100149	14.881395	-0.049101	4.519042
236.284975	7009.196202	14.886400	-0.049079	4.516578
236.401607	7001.123862	14.891405	-0.049096	4.514060
236.171662	6993.028793	14.896410	-0.049048	4.511533
236.093063	6985.009068	14.901415	-0.049028	4.509029
236.224824	6977.082958	14.906419	-0.049048	4.506553
235.949161	6969.040893	14.911424	-0.048991	4.504038
235.999719	6961.096335	14.916429	-0.048996	4.501553
236.006369	6953.076765	14.921434	-0.048992	4.499044
235.900798	6945.083646	14.926439	-0.048967	4.496540
236.050374	6937.067711	14.931443	-0.048990	4.494029
235.974198	6929.029510	14.936448	-0.048971	4.491509
235.965770	6921.058876	14.941453	-0.048964	4.489009
235.554181	6913.086795	14.946458	-0.048883	4.486506
235.647990	6905.030670	14.951463	-0.048895	4.483976
235.598451	6897.106717	14.956467	-0.048881	4.481487
235.345062	6889.025542	14.961472	-0.048829	4.478945
235.508640	6881.088431	14.966477	-0.048854	4.476449
235.503524	6873.009782	14.971482	-0.048848	4.473907
235.631248	6865.009575	14.976487	-0.048867	4.471388
235.431036	6857.042334	14.981491	-0.048825	4.468877
235.486040	6849.010370	14.986496	-0.048830	4.466345
235.394469	6841.029198	14.991501	-0.048808	4.463827
235.245588	6833.067104	14.996506	-0.048775	4.461313
235.342159	6824.992919	15.001511	-0.048788	4.458764
235.326006	6817.088684	15.006515	-0.048780	4.456266
235.014629	6809.025763	15.011520	-0.048717	4.453716
235.004050	6801.025914	15.016525	-0.048710	4.451185
234.990932	6793.003050	15.021530	-0.048703	4.448646
235.014284	6785.024706	15.026535	-0.048702	4.446119
235.007423	6777.040465	15.031539	-0.048696	4.443589
234.803659	6769.010287	15.036544	-0.048653	4.441042
234.993000	6761.055166	15.041549	-0.048683	4.438519
234.984216	6753.021713	15.046554	-0.048676	4.435969
234.936646	6744.976733	15.051559	-0.048662	4.433414
234.929451	6736.968250	15.056563	-0.048656	4.430869
234.703514	6728.970494	15.061568	-0.048609	4.428325
234.908530	6721.013285	15.066573	-0.048642	4.425794
234.756778	6712.980565	15.071578	-0.048609	4.423236
234.669319	6705.007443	15.076583	-0.048588	4.420696
234.648305	6697.017365	15.081587	-0.048579	4.418150
234.475564	6689.000979	15.086592	-0.048541	4.415592
234.676845	6681.003022	15.091597	-0.048574	4.413041
234.536468	6672.946601	15.096602	-0.048543	4.410469
234.549830	6664.970639	15.101607	-0.048540	4.407921
234.570455	6657.000150	15.106611	-0.048539	4.405373
234.500514	6648.969399	15.111616	-0.048521	4.402804
234.423429	6641.003958	15.116621	-0.048502	4.400255
234.327412	6633.027893	15.121626	-0.048479	4.397700
234.293010	6625.000908	15.126631	-0.048467	4.395129
234.232516	6616.995642	15.131635	-0.048451	4.392562
234.087125	6608.919695	15.136640	-0.048419	4.389971
234.225969	6600.953469	15.141645	-0.048440	4.387415
234.087364	6592.974418	15.146650	-0.048409	4.384852
234.003633	6584.999109	15.151655	-0.048388	4.382288
234.001196	6576.978492	15.156659	-0.048383	4.379710
233.985986	6569.014262	15.161664	-0.048375	4.377147
234.051565	6560.999882	15.166669	-0.048382	4.374568
234.257135	6552.966266	15.171674	-0.048416	4.371982
234.106609	6544.935360	15.176679	-0.048382	4.369393
234.086710	6537.016152	15.181683	-0.048374	4.366839
234.051174	6528.946158	15.186688	-0.048362	4.364235
234.057002	6521.041638	15.191693	-0.048358	4.361683
233.877372	6513.002415	15.196698	-0.048320	4.359085
233.976493	6505.045553	15.201703	-0.048333	4.356513
233.918235	6497.007740	15.206707	-0.048317	4.353913
233.604677	6488.842031	15.211712	-0.048254	4.351269
233.627759	6480.910659	15.216717	-0.048253	4.348701
233.501301	6472.911930	15.221722	-0.048225	4.346108
233.444808	6464.946414	15.226727	-0.048209	4.343525
233.286924	6457.004159	15.231731	-0.048175	4.340948
233.252710	6448.967907	15.236736	-0.048163	4.338339
233.378997	6440.966699	15.241741	-0.048182	4.335741
233.202518	6432.940307	15.246746	-0.048144	4.333132
233.016232	6424.931519	15.251751	-0.048104	4.330526
233.179285	6416.957342	15.256755	-0.048130	4.327932
233.119619	6408.932446	15.261760	-0.048113	4.325319
233.164428	6400.983858	15.266765	-0.048117	4.322730
233.131962	6392.957512	15.271770	-0.048106	4.320114
233.095411	6384.967720	15.276775	-0.048094	4.317507
233.003369	6376.971619	15.281779	-0.048072	4.314897
232.845999	6368.919794	15.286784	-0.048037	4.312267
232.969260	6360.899817	15.291789	-0.048055	4.309647
232.744545	6352.972114	15.296794	-0.048008	4.307053
232.881437	6344.897584	15.301799	-0.048029	4.304413
232.949909	6336.954498	15.306803	-0.048037	4.301813
232.851559	6328.919226	15.311808	-0.048013	4.299180
232.852729	6320.968391	15.316813	-0.048009	4.296574
232.625058	6312.942358	15.321818	-0.047961	4.293940
232.453646	6304.898082	15.326823	-0.047924	4.291299
232.397277	6296.904439	15.331827	-0.047909	4.288674
232.315247	6288.906868	15.336832	-0.047888	4.286045
232.512136	6280.898632	15.341837	-0.047920	4.283414
232.344306	6272.953890	15.346842	-0.047884	4.280799
232.298919	6264.951195	15.351847	-0.047870	4.278164
232.444662	6256.975034	15.356851	-0.047892	4.275538
232.123604	6248.878598	15.361856	-0.047828	4.272867
232.395219	6240.853162	15.366861	-0.047873	4.270223
232.185451	6232.876561	15.371866	-0.047829	4.267589
232.066253	6224.884601	15.376871	-0.047802	4.264949
232.019129	6216.966553	15.381875	-0.047788	4.262332
231.997218	6208.903554	15.386880	-0.047779	4.259666
232.073811	6200.938219	15.391885	-0.047788	4.257032
232.031274	6192.892436	15.396890	-0.047775	4.254368
231.825126	6184.929737	15.401895	-0.047732	4.251729
231.813297	6176.905453	15.406899	-0.047725	4.249069
231.725273	6168.921279	15.411904	-0.047703	4.246421
231.798463	6160.917827	15.416909	-0.047712	4.243765
231.796789	6152.941229	15.421914	-0.047707	4.241117
231.702505	6144.889614	15.426919	-0.047684	4.238441
231.774963	6136.990396	15.431923	-0.047693	4.235815
231.568103	6128.916531	15.436928	-0.047649	4.233127
231.878056	6120.903107	15.441933	-0.047702	4.230462
231.639926	6112.908852	15.446938	-0.047652	4.227797
231.572103	6104.901594	15.451943	-0.047635	4.225127
231.614353	6096.950427	15.456947	-0.047638	4.222476
231.416823	6088.920722	15.461952	-0.047596	4.219794
231.561445	6080.987753	15.466957	-0.047618	4.217146
231.548501	6072.900120	15.471962	-0.047610	4.214444
231.301243	6064.923785	15.476967	-0.047559	4.211774
231.321140	6056.936938	15.481971	-0.047558	4.209102
231.328207	6048.955558	15.486976	-0.047554	4.206430
231.222377	6040.931533	15.491981	-0.047529	4.203740
231.244244	6032.950586	15.496986	-0.047528	4.201065
231.098143	6024.957687	15.501991	-0.047496	4.198382
231.251996	6016.969747	15.506995	-0.047520	4.195703
231.252396	6008.857018	15.512000	-0.047515	4.192978
231.092969	6000.816918	15.517005	-0.047480	4.190274
231.210951	5992.867774	15.522010	-0.047497	4.187602
231.245770	5984.854028	15.527015	-0.047499	4.184905
231.097240	5976.933920	15.532019	-0.047466	4.182237
230.936763	5968.894288	15.537024	-0.047431	4.179526
231.152066	5960.916937	15.542029	-0.047466	4.176838
231.076154	5952.908077	15.547034	-0.047447	4.174135
230.839497	5944.896881	15.552039	-0.047398	4.171428
231.066650	5936.902169	15.557043	-0.047435	4.168730
230.735870	5928.888967	15.562048	-0.047369	4.166017
230.734642	5920.927109	15.567053	-0.047363	4.163324
230.777395	5912.914507	15.572058	-0.047366	4.160612
230.669859	5904.921507	15.577063	-0.047341	4.157903
230.578974	5896.916615	15.582067	-0.047319	4.155189
230.437665	5888.857103	15.587072	-0.047288	4.152454
230.451528	5880.849948	15.592077	-0.047285	4.149736
230.461899	5872.905139	15.597082	-0.047282	4.147038
230.452896	5864.881699	15.602087	-0.047276	4.144312
230.522349	5856.913070	15.607091	-0.047284	4.141603
230.492206	5848.888997	15.612096	-0.047273	4.138872
230.426061	5840.933859	15.617101	-0.047256	4.136162
230.285210	5832.893244	15.622106	-0.047224	4.133421
230.201093	5824.855965	15.627111	-0.047204	4.130679
230.269439	5816.881606	15.632115	-0.047211	4.127959
230.112577	5808.894249	15.637120	-0.047177	4.125230
230.374105	5800.921457	15.642125	-0.047221	4.122510
230.230701	5792.883964	15.647130	-0.047189	4.119760
229.887882	5784.949666	15.652135	-0.047120	4.117042
230.089586	5776.905506	15.657139	-0.047153	4.114291
229.658734	5768.853158	15.662144	-0.047068	4.111527
229.660727	5760.869208	15.667149	-0.047063	4.108790
229.707211	5752.883428	15.672154	-0.047067	4.106051
229.833395	5744.889001	15.677159	-0.047085	4.103309
229.737698	5736.896602	15.682163	-0.047062	4.100563
229.511931	5728.902833	15.687168	-0.047015	4.097812
229.652531	5720.913896	15.692173	-0.047036	4.095066
229.649711	5712.920456	15.697178	-0.047031	4.092315
229.526527	5704.884566	15.702183	-0.047003	4.089546
229.612055	5696.956421	15.707187	-0.047014	4.086815
229.430519	5688.893008	15.712192	-0.046975	4.084032
229.554554	5680.965885	15.717197	-0.046993	4.081298
229.448246	5672.943900	15.722202	-0.046968	4.078526
229.602741	5664.952147	15.727207	-0.046992	4.075766
229.602524	5656.925976	15.732211	-0.046987	4.072991
229.349879	5648.909224	15.737216	-0.046935	4.070213
229.278173	5640.933932	15.742221	-0.046917	4.067451
229.209097	5632.918054	15.747226	-0.046899	4.064672
228.938133	5624.955613	15.752231	-0.046843	4.061907
228.985386	5616.952260	15.757235	-0.046847	4.059131
228.883322	5608.952492	15.762240	-0.046823	4.056352
229.155121	5600.941735	15.767245	-0.046869	4.053572
228.989283	5592.936787	15.772250	-0.046833	4.050786
228.900696	5584.896491	15.777255	-0.046811	4.047987
229.032489	5576.931341	15.782259	-0.046831	4.045216
228.992021	5568.975350	15.787264	-0.046818	4.042443
228.862817	5560.923012	15.792269	-0.046789	4.039634
228.842140	5552.979014	15.797274	-0.046780	4.036862
228.783755	5544.902672	15.802279	-0.046764	4.034041
228.670430	5536.856722	15.807283	-0.046738	4.031228
228.623056	5528.868020	15.812288	-0.046724	4.028434
228.561710	5520.881930	15.817293	-0.046708	4.025639
228.468535	5512.932232	15.822298	-0.046686	4.022854
228.398997	5504.883715	15.827303	-0.046668	4.020033
228.656685	5496.937652	15.832307	-0.046711	4.017251
228.451421	5488.886835	15.837312	-0.046667	4.014423
228.162886	5480.899726	15.842317	-0.046609	4.011615
228.230163	5472.916581	15.847322	-0.046616	4.008811
228.294889	5464.891183	15.852327	-0.046623	4.005990
228.125425	5456.956527	15.857331	-0.046587	4.003195
227.991570	5448.923050	15.862336	-0.046557	4.000365
228.009026	5440.967246	15.867341	-0.046555	3.997562
228.014653	5432.940558	15.872346	-0.046551	3.994732
227.993898	5424.876553	15.877351	-0.046542	3.991886
228.119512	5416.880486	15.882355	-0.046560	3.989065
228.090686	5408.891903	15.887360	-0.046550	3.986241
227.969584	5400.882408	15.892365	-0.046522	3.983407
228.088240	5392.935359	15.897370	-0.046540	3.980597
227.987289	5384.946914	15.902375	-0.046516	3.977767
228.040199	5376.936685	15.907379	-0.046521	3.974929
227.727824	5368.904590	15.912384	-0.046457	3.972076
227.738074	5360.889434	15.917389	-0.046454	3.969232
227.792174	5352.935933	15.922394	-0.046459	3.966408
227.532932	5344.947785	15.927399	-0.046406	3.963565
227.660676	5336.994232	15.932403	-0.046425	3.960738
227.513526	5329.001727	15.937408	-0.046392	3.957891
227.362441	5320.973171	15.942413	-0.046359	3.955030
227.595817	5312.922121	15.947418	-0.046398	3.952164
227.523480	5304.917156	15.952423	-0.046379	3.949308
227.372296	5296.962116	15.957427	-0.046346	3.946466
227.369786	5288.954865	15.962432	-0.046341	3.943606
227.281535	5280.990855	15.967437	-0.046319	3.940758
227.156349	5273.017905	15.972442	-0.046291	3.937903
226.969140	5264.951014	15.977447	-0.046251	3.935012
227.099539	5256.979638	15.982451	-0.046270	3.932159
227.180235	5248.942501	15.987456	-0.046280	3.929280
226.933754	5240.991253	15.992461	-0.046229	3.926423
226.911395	5232.996295	15.997466	-0.046220	3.923552
226.781412	5224.986620	16.002471	-0.046191	3.920672
226.788767	5217.042714	16.007475	-0.046187	3.917816
226.706815	5208.992955	16.012480	-0.046167	3.914918
226.936300	5200.960907	16.017485	-0.046205	3.912030
226.836795	5192.956022	16.022490	-0.046181	3.909144
226.733429	5185.006628	16.027495	-0.046157	3.906275
226.909008	5177.008827	16.032499	-0.046185	3.903393
226.720434	5168.995271	16.037504	-0.046144	3.900495
226.594718	5161.001731	16.042509	-0.046116	3.897604
226.459080	5153.028511	16.047514	-0.046086	3.894717
226.532497	5144.967449	16.052519	-0.046094	3.891801
226.575070	5137.013985	16.057523	-0.046097	3.888921
226.270464	5129.015133	16.062528	-0.046036	3.886016
226.404125	5121.010183	16.067533	-0.046055	3.883114
226.392819	5113.000881	16.072538	-0.046048	3.880207
226.190871	5104.998398	16.077543	-0.046006	3.877295
226.209503	5097.028738	16.082547	-0.046004	3.874398
226.261126	5088.742468	16.087552	-0.046009	3.871384
226.096950	5080.846323	16.092557	-0.045973	3.868506
225.960356	5072.876693	16.097562	-0.045943	3.865599
226.206178	5064.937541	16.102567	-0.045983	3.862708
226.133654	5056.971271	16.107571	-0.045965	3.859800
225.748022	5049.015489	16.112576	-0.045888	3.856886
225.684640	5041.012200	16.117581	-0.045871	3.853960
225.913961	5032.959526	16.122586	-0.045909	3.851019
225.742378	5024.956562	16.127591	-0.045872	3.848086
225.791669	5017.014727	16.132595	-0.045876	3.845177
225.935085	5009.007211	16.137600	-0.045898	3.842244
225.995708	5001.016368	16.142605	-0.045904	3.839314
225.641175	4993.105203	16.147610	-0.045833	3.836402
225.575085	4985.052218	16.152615	-0.045816	3.833441
225.605369	4977.054318	16.157619	-0.045816	3.830500
225.512588	4969.029723	16.162624	-0.045794	3.827545
225.408155	4961.033221	16.167629	-0.045770	3.824598
225.590467	4953.065405	16.172634	-0.045799	3.821664
225.508756	4945.036793	16.177639	-0.045778	3.818701
225.303646	4937.091755	16.182643	-0.045735	3.815764
225.296204	4929.078951	16.187648	-0.045729	3.812803
225.395804	4921.045047	16.192653	-0.045742	3.809835
225.386982	4913.089485	16.197658	-0.045736	3.806890
225.285099	4905.083180	16.202663	-0.045712	3.803923
225.433440	4897.120665	16.207667	-0.045734	3.800976
225.219777	4889.134302	16.212672	-0.045690	3.798009
225.192649	4881.094474	16.217677	-0.045679	3.795024
225.179783	4873.081984	16.222682	-0.045672	3.792047
225.059476	4865.025119	16.227687	-0.045645	3.789049
224.885410	4857.095327	16.232691	-0.045607	3.786095
224.908261	4849.072836	16.237696	-0.045606	3.783108
225.007733	4841.083051	16.242701	-0.045620	3.780132
224.981369	4833.102095	16.247706	-0.045610	3.777155
224.743542	4825.080889	16.252711	-0.045561	3.774156
224.966027	4817.117574	16.257715	-0.045597	3.771186
224.836357	4809.055850	16.262720	-0.045568	3.768170
224.648323	4801.060097	16.267725	-0.045528	3.765174
224.947158	4793.116782	16.272730	-0.045579	3.762206
224.766932	4785.120806	16.277735	-0.045540	3.759206
224.421699	4777.194735	16.282739	-0.045471	3.756225
224.528757	4769.118241	16.287744	-0.045486	3.753196
224.618140	4761.084215	16.292749	-0.045497	3.750180
224.779760	4753.077853	16.297754	-0.045522	3.747174
224.340291	4745.099650	16.302759	-0.045436	3.744162
224.484463	4737.122977	16.307763	-0.045457	3.741162
224.224344	4729.123409	16.312768	-0.045404	3.738141
224.152031	4721.119412	16.317773	-0.045385	3.735120
224.314230	4713.126933	16.322778	-0.045411	3.732107
224.192252	4705.120876	16.327783	-0.045383	3.729080
224.161157	4697.181628	16.332787	-0.045372	3.726077
224.047646	4689.159214	16.337792	-0.045346	3.723039
224.272335	4681.142352	16.342797	-0.045383	3.720009
224.149039	4673.235794	16.347802	-0.045355	3.717009
224.036155	4665.168818	16.352807	-0.045329	3.713946
224.306586	4657.077208	16.357811	-0.045374	3.710881
224.126934	4649.096904	16.362816	-0.045336	3.707845
223.884450	4641.148644	16.367821	-0.045285	3.704816
223.936085	4633.196021	16.372826	-0.045290	3.701791
223.882962	4625.180532	16.377831	-0.045275	3.698737
223.818741	4617.229728	16.382835	-0.045258	3.695704
223.722284	4609.207441	16.387840	-0.045235	3.692641
223.604852	4601.197328	16.392845	-0.045208	3.689580
223.594389	4593.231759	16.397850	-0.045201	3.686536
223.386766	4585.218954	16.402855	-0.045158	3.683466
223.664505	4577.247479	16.407859	-0.045204	3.680422
223.715678	4569.247100	16.412864	-0.045209	3.677358
223.355853	4561.238555	16.417869	-0.045137	3.674278
223.283522	4553.232231	16.422874	-0.045118	3.671204
223.442493	4545.211392	16.427879	-0.045143	3.668127
223.312187	4537.241914	16.432883	-0.045114	3.665061
223.397710	4529.240222	16.437888	-0.045125	3.661985
223.450482	4521.232046	16.442893	-0.045129	3.658903
223.320749	4513.293234	16.447898	-0.045100	3.655840
223.241451	4505.241181	16.452903	-0.045081	3.652732
223.239681	4497.224665	16.457907	-0.045075	3.649638
223.221127	4489.235494	16.462912	-0.045067	3.646551
222.964945	4481.263816	16.467917	-0.045014	3.643461
222.887524	4473.304414	16.472922	-0.044995	3.640379
222.839276	4465.295793	16.477927	-0.044981	3.637276
222.714290	4457.303387	16.482931	-0.044952	3.634174
222.660356	4449.250182	16.487936	-0.044937	3.631048
222.879420	4441.238719	16.492941	-0.044973	3.627943
222.975189	4433.251489	16.497946	-0.044986	3.624841
222.665613	4425.302730	16.502951	-0.044923	3.621741
222.707388	4417.300112	16.507955	-0.044926	3.618626
222.644656	4409.320559	16.512960	-0.044909	3.615515
222.640410	4401.322963	16.517965	-0.044903	3.612396
222.664367	4393.283911	16.522970	-0.044903	3.609259
222.681717	4385.298641	16.527975	-0.044901	3.606139
222.598919	4377.340995	16.532979	-0.044881	3.603026
222.496381	4369.371747	16.537984	-0.044857	3.599904
222.428546	4361.398210	16.542989	-0.044839	3.596779
222.477132	4353.388237	16.547994	-0.044843	3.593640
222.354556	4345.328405	16.552999	-0.044815	3.590474
222.201452	4337.382837	16.558003	-0.044782	3.587349
222.210915	4329.375313	16.563008	-0.044778	3.584202
222.042224	4321.399680	16.568013	-0.044742	3.581059
222.026374	4313.408887	16.573018	-0.044734	3.577912
221.965905	4305.418898	16.578023	-0.044718	3.574761
221.919070	4297.433404	16.583027	-0.044704	3.571610
221.783786	4289.403787	16.588032	-0.044674	3.568436
221.790722	4281.400118	16.593037	-0.044670	3.565273
221.684023	4273.437197	16.598042	-0.044645	3.562121
221.601680	4265.439371	16.603047	-0.044625	3.558952
221.778565	4257.457809	16.608051	-0.044653	3.555795
221.891790	4249.355805	16.613056	-0.044669	3.552585
221.761437	4241.339800	16.618061	-0.044639	3.549400
221.740108	4233.402225	16.623066	-0.044631	3.546245
221.585968	4225.400864	16.628071	-0.044597	3.543059
221.776714	4217.426300	16.633075	-0.044627	3.539891
221.399710	4209.438173	16.638080	-0.044552	3.536697
221.371867	4201.423203	16.643085	-0.044542	3.533501
221.471043	4193.435586	16.648090	-0.044555	3.530316
221.325952	4185.438550	16.653095	-0.044523	3.527117
221.392104	4177.447571	16.658099	-0.044531	3.523924
221.298174	4169.489296	16.663104	-0.044508	3.520737
221.097738	4161.503584	16.668109	-0.044466	3.517532
221.145462	4153.515531	16.673114	-0.044470	3.514331
221.155801	4145.467627	16.678119	-0.044467	3.511102
221.197740	4137.470528	16.683123	-0.044469	3.507891
220.939774	4129.484534	16.688128	-0.044416	3.504673
220.847167	4121.522642	16.693133	-0.044394	3.501466
221.023890	4113.542500	16.698138	-0.044422	3.498258
220.781607	4105.544208	16.703143	-0.044372	3.495026
220.833246	4097.552890	16.708147	-0.044377	3.491803
221.114057	4089.512345	16.713152	-0.044424	3.488565
221.109359	4081.523950	16.718157	-0.044418	3.485335
220.776161	4073.625125	16.723162	-0.044351	3.482129
220.750468	4065.594661	16.728167	-0.044341	3.478875
220.766351	4057.616932	16.733171	-0.044339	3.475642
220.653352	4049.597627	16.738176	-0.044313	3.472384
220.482705	4041.574351	16.743181	-0.044276	3.469120
220.594089	4033.579222	16.748186	-0.044292	3.465874
220.250248	4025.622534	16.753191	-0.044223	3.462625
220.329870	4017.622711	16.758195	-0.044233	3.459369
220.340737	4009.655808	16.763200	-0.044230	3.456122
220.415438	4001.594900	16.768205	-0.044239	3.452835
220.465071	3993.600196	16.773210	-0.044243	3.449571
220.309921	3985.602882	16.778215	-0.044209	3.446297
220.431090	3977.664056	16.783219	-0.044226	3.443052
220.117376	3969.647622	16.788224	-0.044163	3.439758
220.073792	3961.721290	16.793229	-0.044150	3.436507
220.138532	3953.691752	16.798234	-0.044157	3.433214
220.082782	3945.641010	16.803239	-0.044142	3.429905
220.018740	3937.654148	16.808243	-0.044125	3.426618
220.076627	3929.681638	16.813248	-0.044130	3.423339
220.039694	3921.681383	16.818253	-0.044118	3.420042
219.902565	3913.752380	16.823258	-0.044088	3.416767
219.967899	3905.688036	16.828263	-0.044095	3.413441
219.827139	3897.703761	16.833267	-0.044064	3.410137
219.512750	3889.737961	16.838272	-0.044000	3.406832
219.554976	3881.741270	16.843277	-0.044003	3.403523
219.611652	3873.792549	16.848282	-0.044009	3.400231
219.361782	3865.806460	16.853287	-0.043957	3.396910
219.412274	3857.776033	16.858291	-0.043962	3.393578
219.453740	3849.697172	16.863296	-0.043964	3.390221
219.591904	3841.693148	16.868301	-0.043985	3.386896
219.458632	3833.762579	16.873306	-0.043955	3.383589
219.295638	3825.768236	16.878311	-0.043920	3.380251
219.269633	3817.834555	16.883315	-0.043910	3.376940
219.189033	3809.810214	16.888320	-0.043890	3.373586
219.136029	3801.798260	16.893325	-0.043875	3.370234
219.202571	3793.822857	16.898330	-0.043882	3.366899
219.045539	3785.839476	16.903335	-0.043848	3.363549
218.797852	3777.895724	16.908339	-0.043797	3.360209
218.910993	3769.870206	16.913344	-0.043813	3.356845
219.045553	3761.840440	16.918349	-0.043833	3.353476
218.935772	3753.859840	16.923354	-0.043808	3.350115
218.771006	3745.885396	16.928359	-0.043772	3.346752
218.854768	3737.893026	16.933363	-0.043783	3.343387
218.863970	3729.907760	16.938368	-0.043779	3.340018
218.998392	3721.917410	16.943373	-0.043799	3.336649
219.024273	3713.927580	16.948378	-0.043799	3.333273
218.806153	3705.897160	16.953383	-0.043754	3.329867
218.681375	3697.957478	16.958387	-0.043725	3.326499
218.751613	3689.943978	16.963392	-0.043733	3.323104
218.716840	3681.940547	16.968397	-0.043722	3.319705
218.492384	3674.043616	16.973402	-0.043675	3.316342
218.374558	3665.989092	16.978407	-0.043648	3.312912
218.606801	3657.939745	16.983411	-0.043686	3.309493
218.532059	3649.985953	16.988416	-0.043667	3.306101
218.239108	3642.025444	16.993421	-0.043608	3.302693
218.268296	3634.033551	16.998426	-0.043608	3.299281
218.306660	3626.047634	17.003431	-0.043610	3.295869
218.005360	3618.069831	17.008435	-0.043549	3.292443
218.007976	3610.042557	17.013440	-0.043545	3.289004
218.022165	3602.054652	17.018445	-0.043542	3.285579
218.130672	3594.095628	17.023450	-0.043558	3.282166
217.993278	3586.100291	17.028455	-0.043527	3.278725
218.038773	3578.135271	17.033459	-0.043531	3.275300
217.872571	3570.114483	17.038464	-0.043495	3.271839
217.594164	3562.115381	17.043469	-0.043438	3.268380
217.847652	3554.096578	17.048474	-0.043480	3.264929
217.651764	3546.136629	17.053479	-0.043438	3.261482
217.613473	3538.164974	17.058483	-0.043426	3.258033
217.519988	3530.169376	17.063488	-0.043404	3.254568
217.552759	3522.141923	17.068493	-0.043405	3.251090
217.582511	3514.183735	17.073498	-0.043405	3.247638
217.528609	3506.159115	17.078503	-0.043390	3.244150
217.427567	3498.241528	17.083507	-0.043367	3.240704
217.289780	3490.261274	17.088512	-0.043336	3.237225
217.340722	3482.221989	17.093517	-0.043340	3.233724
217.461431	3474.159849	17.098522	-0.043358	3.230212
217.356404	3466.161089	17.103527	-0.043333	3.226714
217.338017	3458.206485	17.108531	-0.043325	3.223236
217.374202	3450.243953	17.113536	-0.043327	3.219753
217.302783	3442.253843	17.118541	-0.043308	3.216249
217.297833	3434.277599	17.123546	-0.043302	3.212751
217.006028	3426.281690	17.128551	-0.043243	3.209228
216.969476	3418.337296	17.133555	-0.043231	3.205734
216.961365	3410.358469	17.138560	-0.043225	3.202223
216.977044	3402.356393	17.143565	-0.043223	3.198699
216.945169	3394.378269	17.148570	-0.043212	3.195179
216.822531	3386.351174	17.153575	-0.043184	3.191630
216.803577	3378.356346	17.158579	-0.043175	3.188095
216.692737	3370.356626	17.163584	-0.043150	3.184551
216.637412	3362.401399	17.168589	-0.043134	3.181025
216.681619	3354.415203	17.173594	-0.043138	3.177485
216.459515	3346.422769	17.178599	-0.043091	3.173927
216.507327	3338.402133	17.183603	-0.043095	3.170364
216.656593	3330.422054	17.188608	-0.043118	3.166820
216.510449	3322.419220	17.193613	-0.043086	3.163249
216.323615	3314.484721	17.198618	-0.043046	3.159702
216.376892	3306.496734	17.203623	-0.043051	3.156138
216.281001	3298.492495	17.208627	-0.043028	3.152556
216.210078	3290.487991	17.213632	-0.043010	3.148971
216.218965	3282.465331	17.218637	-0.043006	3.145377
216.308415	3274.516985	17.223642	-0.043018	3.141816
216.068832	3266.525849	17.228647	-0.042968	3.138218
216.261271	3258.554230	17.233651	-0.042999	3.134643
216.285780	3250.552015	17.238656	-0.042999	3.131042
215.916032	3242.571637	17.243661	-0.042925	3.127430
215.996052	3234.608014	17.248666	-0.042935	3.123842
215.995313	3226.618680	17.253671	-0.042930	3.120233
215.850536	3218.666708	17.258675	-0.042898	3.116632
215.824945	3210.652166	17.263680	-0.042888	3.113003
215.788838	3202.632887	17.268685	-0.042876	3.109367
215.856000	3194.652570	17.273690	-0.042884	3.105749
215.689047	3186.696727	17.278695	-0.042848	3.102127
215.742517	3178.706185	17.283699	-0.042853	3.098496
215.649225	3170.707536	17.288704	-0.042830	3.094850
215.496963	3162.716089	17.293709	-0.042797	3.091200
215.628564	3154.730803	17.298714	-0.042816	3.087561
215.347547	3146.744014	17.303719	-0.042759	3.083899
215.507834	3138.773977	17.308723	-0.042784	3.080260
215.436511	3130.808860	17.313728	-0.042766	3.076609
215.148112	3122.760329	17.318733	-0.042707	3.072904
215.281918	3114.721441	17.323738	-0.042727	3.069220
215.249176	3106.758693	17.328743	-0.042716	3.065558
215.037610	3098.816990	17.333747	-0.042671	3.061893
215.228773	3090.820610	17.338752	-0.042702	3.058218
215.093572	3082.842233	17.343757	-0.042672	3.054531
215.035882	3074.889229	17.348762	-0.042656	3.050854
214.998060	3066.881049	17.353767	-0.042644	3.047149
215.101686	3058.886893	17.358771	-0.042658	3.043453
214.879896	3050.939425	17.363776	-0.042612	3.039758
214.838701	3042.974281	17.368781	-0.042599	3.036059
215.049944	3034.936929	17.373786	-0.042633	3.032334
214.820845	3026.944423	17.378791	-0.042586	3.028604
214.750185	3018.962114	17.383795	-0.042568	3.024882
214.986022	3010.993787	17.388800	-0.042607	3.021177
214.841718	3003.011411	17.393805	-0.042575	3.017442
214.742329	2995.040958	17.398810	-0.042551	3.013710
214.734981	2987.031448	17.403815	-0.042545	3.009960
214.783780	2979.065290	17.408819	-0.042549	3.006228
214.556139	2971.105555	17.413824	-0.042501	3.002481
214.460942	2963.119983	17.418829	-0.042479	2.998724
214.504072	2955.157028	17.423834	-0.042482	2.994980
214.357838	2947.127383	17.428839	-0.042450	2.991189
214.243342	2939.154230	17.433843	-0.042423	2.987423
214.353786	2931.150759	17.438848	-0.042439	2.983648
214.143369	2923.187582	17.443853	-0.042395	2.979872
214.126639	2915.231071	17.448858	-0.042386	2.976104
213.991099	2907.222329	17.453863	-0.042356	2.972300
214.039965	2899.229791	17.458867	-0.042360	2.968508
213.947563	2891.254065	17.463872	-0.042338	2.964712
213.865532	2883.301910	17.468877	-0.042318	2.960924
214.023652	2875.307272	17.473882	-0.042342	2.957122
213.878446	2867.290825	17.478887	-0.042310	2.953289
213.659967	2859.325429	17.483891	-0.042265	2.949472
213.922277	2851.323624	17.488896	-0.042308	2.945658
213.839174	2843.340851	17.493901	-0.042288	2.941830
213.660323	2835.415994	17.498906	-0.042250	2.938019
213.457607	2827.430703	17.503911	-0.042207	2.934174
213.669432	2819.406895	17.508915	-0.042241	2.930326
213.459971	2811.447306	17.513920	-0.042197	2.926482
213.316522	2803.467768	17.518925	-0.042166	2.922627
213.459400	2795.501697	17.523930	-0.042187	2.918789
213.512530	2787.481025	17.528935	-0.042192	2.914914
213.346688	2779.439651	17.533939	-0.042156	2.911012
213.409834	2771.454067	17.538944	-0.042163	2.907145
213.324792	2763.478724	17.543949	-0.042142	2.903269
213.418909	2755.544331	17.548954	-0.042155	2.899418
213.265916	2747.559340	17.553959	-0.042121	2.895524
213.280141	2739.583902	17.558963	-0.042119	2.891638
213.023499	2731.631386	17.563968	-0.042066	2.887743
212.830135	2723.646298	17.568973	-0.042025	2.883830
213.006484	2715.675541	17.573978	-0.042053	2.879940
212.994497	2707.688750	17.578983	-0.042046	2.876026
212.947265	2699.689441	17.583987	-0.042032	2.872098
212.853518	2691.716475	17.588992	-0.042009	2.868176
212.935174	2683.696718	17.593997	-0.042019	2.864234
212.905596	2675.780891	17.599002	-0.042009	2.860333
212.659956	2667.791463	17.604007	-0.041958	2.856378
212.769155	2659.806642	17.609011	-0.041974	2.852439
212.752479	2651.819910	17.614016	-0.041965	2.848487
212.148118	2643.856688	17.619021	-0.041848	2.844508
212.348196	2635.902948	17.624026	-0.041880	2.840573
212.615056	2627.911083	17.629031	-0.041925	2.836618
212.436543	2619.896897	17.634035	-0.041887	2.832621
212.329984	2611.901569	17.639040	-0.041862	2.828631
212.225541	2603.930467	17.644045	-0.041837	2.824649
212.208037	2595.985692	17.649050	-0.041829	2.820678
212.092066	2587.999796	17.654055	-0.041803	2.816676
212.007317	2580.008029	17.659059	-0.041782	2.812667
212.214026	2572.001018	17.664064	-0.041815	2.808662
211.906719	2564.032869	17.669069	-0.041753	2.804640
212.128302	2556.095261	17.674074	-0.041789	2.800659
211.950026	2548.118456	17.679079	-0.041751	2.796629
211.932915	2540.120984	17.684083	-0.041743	2.792593
211.811210	2532.134252	17.689088	-0.041715	2.788549
211.664815	2524.150325	17.694093	-0.041683	2.784500
211.623673	2516.215086	17.699098	-0.041670	2.780476
211.734089	2508.226978	17.704103	-0.041686	2.776428
211.785362	2500.227903	17.709107	-0.041690	2.772365
211.770851	2492.251281	17.714112	-0.041683	2.768303
211.418308	2484.288028	17.719117	-0.041612	2.764223
211.512726	2476.342334	17.724122	-0.041625	2.760172
211.513683	2468.355172	17.729127	-0.041620	2.756088
211.538973	2460.302049	17.734131	-0.041619	2.751965
211.433643	2452.329907	17.739136	-0.041595	2.747871
211.164518	2444.365970	17.744141	-0.041540	2.743764
211.149469	2436.415585	17.749146	-0.041532	2.739673
211.038398	2428.452124	17.754151	-0.041506	2.735564
211.066594	2420.459369	17.759155	-0.041507	2.731442
211.146269	2412.474353	17.764160	-0.041516	2.727321
210.961806	2404.513518	17.769165	-0.041477	2.723190
210.861297	2396.571104	17.774170	-0.041453	2.719068
210.900857	2388.595210	17.779175	-0.041456	2.714930
210.949510	2380.596159	17.784179	-0.041460	2.710775
210.830372	2372.631846	17.789184	-0.041433	2.706620
210.743859	2364.650186	17.794189	-0.041411	2.702453
210.790278	2356.690587	17.799194	-0.041415	2.698299
210.619203	2348.722292	17.804199	-0.041378	2.694120
210.628795	2340.715487	17.809203	-0.041375	2.689926
210.631858	2332.770107	17.814208	-0.041371	2.685757
210.549479	2324.782694	17.819213	-0.041350	2.681554
210.501716	2316.845139	17.824218	-0.041336	2.677373
210.417397	2308.850477	17.829223	-0.041316	2.673153
210.409783	2300.834346	17.834227	-0.041309	2.668920
210.324396	2292.890542	17.839232	-0.041288	2.664714
210.284322	2284.904332	17.844237	-0.041276	2.660481
210.247551	2276.962787	17.849242	-0.041264	2.656265
210.174910	2268.954894	17.854247	-0.041246	2.652005
210.039380	2261.003365	17.859251	-0.041215	2.647764
210.170361	2253.034283	17.864256	-0.041235	2.643524
210.148054	2245.058190	17.869261	-0.041226	2.639264
210.302590	2237.121916	17.874266	-0.041249	2.635030
210.174899	2229.116345	17.879271	-0.041221	2.630733
209.920824	2221.156393	17.884275	-0.041168	2.626445
209.955633	2213.197940	17.889280	-0.041170	2.622171
209.841431	2205.223093	17.894285	-0.041143	2.617870
209.828343	2197.266513	17.899290	-0.041136	2.613579
209.587505	2189.274777	17.904295	-0.041086	2.609247
209.583592	2181.316553	17.909299	-0.041080	2.604941
209.652466	2173.348595	17.914304	-0.041088	2.600628
209.602232	2165.383681	17.919309	-0.041074	2.596301
209.587983	2157.298481	17.924314	-0.041066	2.591905
209.388206	2149.285748	17.929319	-0.041024	2.587527
209.514697	2141.323243	17.934323	-0.041043	2.583192
209.397374	2133.409219	17.939328	-0.041016	2.578859
209.449984	2125.435893	17.944333	-0.041021	2.574498
209.427461	2117.480386	17.949338	-0.041011	2.570135
209.300805	2109.527119	17.954343	-0.040983	2.565758
209.187342	2101.595464	17.959347	-0.040957	2.561386
209.228729	2093.640268	17.964352	-0.040959	2.557004
209.159446	2085.657335	17.969357	-0.040942	2.552592
209.172866	2077.705941	17.974362	-0.040939	2.548196
209.076219	2069.730450	17.979367	-0.040916	2.543771
209.143174	2061.753115	17.984371	-0.040924	2.539349
208.977777	2053.820386	17.989376	-0.040888	2.534927
208.629833	2045.849295	17.994381	-0.040818	2.530463
208.806584	2037.876233	17.999386	-0.040846	2.526028
208.633485	2029.932303	18.004391	-0.040809	2.521576
208.505034	2021.986465	18.009395	-0.040780	2.517118
208.703259	2013.981930	18.014400	-0.040812	2.512643
208.597590	2005.979285	18.019405	-0.040787	2.508139
208.557176	1998.019236	18.024410	-0.040774	2.503655
208.351994	1990.076202	18.029415	-0.040731	2.499162
208.388064	1982.120527	18.034419	-0.040733	2.494670
208.488123	1974.120160	18.039424	-0.040747	2.490150
208.296612	1966.170678	18.044429	-0.040706	2.485629
208.472501	1958.211953	18.049434	-0.040734	2.481122
208.126101	1950.293833	18.054439	-0.040664	2.476591
207.926953	1942.318162	18.059443	-0.040622	2.472029
207.991408	1934.336600	18.064448	-0.040629	2.467476
208.054880	1926.355135	18.069453	-0.040636	2.462914
207.912293	1918.428696	18.074458	-0.040604	2.458359
207.737421	1910.474821	18.079463	-0.040567	2.453778
207.923909	1902.455425	18.084467	-0.040597	2.449178
207.680307	1894.542378	18.089472	-0.040546	2.444598
207.700331	1886.575324	18.094477	-0.040545	2.439998
207.718575	1878.634018	18.099482	-0.040543	2.435404
207.529274	1870.588459	18.104487	-0.040503	2.430726
207.586638	1862.604300	18.109491	-0.040509	2.426092
207.685774	1854.661708	18.114496	-0.040522	2.421478
207.625301	1846.714151	18.119501	-0.040506	2.416839
207.351614	1838.792297	18.124506	-0.040450	2.412190
207.173678	1830.823067	18.129511	-0.040412	2.407512
207.359894	1822.832921	18.134515	-0.040442	2.402840
207.393260	1814.905101	18.139520	-0.040443	2.398184
207.332847	1806.955104	18.144525	-0.040427	2.393499
207.327672	1798.975780	18.149530	-0.040421	2.388791
207.426113	1790.992237	18.154535	-0.040434	2.384080
207.255199	1783.078948	18.159539	-0.040397	2.379380
207.274694	1775.139537	18.164544	-0.040396	2.374670
207.196041	1767.154044	18.169549	-0.040376	2.369916
207.025955	1759.228862	18.174554	-0.040340	2.365180
206.705620	1751.296291	18.179559	-0.040275	2.360419
206.932305	1743.304491	18.184563	-0.040312	2.355656
207.145156	1735.312873	18.189568	-0.040347	2.350883
206.775989	1727.380069	18.194573	-0.040273	2.346088
206.624694	1719.460075	18.199578	-0.040240	2.341309
206.628563	1711.479161	18.204583	-0.040236	2.336496
206.625231	1703.519786	18.209587	-0.040230	2.331686
206.564182	1695.572071	18.214592	-0.040214	2.326868
206.388828	1687.628428	18.219597	-0.040176	2.322032
206.447682	1679.675346	18.224602	-0.040182	2.317201
206.235376	1671.731620	18.229607	-0.040138	2.312342
206.258459	1663.766352	18.234611	-0.040137	2.307480
206.247043	1655.811111	18.239616	-0.040130	2.302610
206.427266	1647.822725	18.244621	-0.040158	2.297726
206.328563	1639.903254	18.249626	-0.040135	2.292851
206.113503	1631.956704	18.254631	-0.040090	2.287939
205.859102	1624.033791	18.259635	-0.040038	2.283027
205.936106	1616.089627	18.264640	-0.040047	2.278119
206.002907	1608.074125	18.269645	-0.040054	2.273156
206.017806	1600.081751	18.274650	-0.040052	2.268192
205.721505	1592.165037	18.279655	-0.039992	2.263238
205.842819	1584.203600	18.284659	-0.040010	2.258280
205.940688	1576.252335	18.289664	-0.040023	2.253317
205.606858	1568.328377	18.294669	-0.039956	2.248321
205.540862	1560.390602	18.299674	-0.039938	2.243329
205.406660	1552.456027	18.304679	-0.039909	2.238323
205.504021	1544.496769	18.309683	-0.039922	2.233309
205.513061	1536.535367	18.314688	-0.039918	2.228275
205.181479	1528.616576	18.319693	-0.039852	2.223227
205.515007	1520.634127	18.324698	-0.039909	2.218186
205.081337	1512.754434	18.329703	-0.039823	2.213130
205.175835	1504.759541	18.334707	-0.039836	2.208037
205.263964	1496.818037	18.339712	-0.039847	2.202965
205.027412	1488.900456	18.344717	-0.039798	2.197867
205.150122	1480.936772	18.349722	-0.039816	2.192761
205.130317	1472.953130	18.354727	-0.039807	2.187617
204.981031	1465.028114	18.359731	-0.039774	2.182487
204.934731	1457.118042	18.364736	-0.039761	2.177364
204.815209	1449.151206	18.369741	-0.039734	2.172185
204.947408	1441.200937	18.374746	-0.039753	2.167027
204.806780	1433.272246	18.379751	-0.039722	2.161847
204.712430	1425.355325	18.384755	-0.039700	2.156665
204.677531	1417.417797	18.389760	-0.039688	2.151464
204.520612	1409.465639	18.394765	-0.039654	2.146228
204.526976	1401.524032	18.399770	-0.039650	2.141002
204.505358	1393.598008	18.404775	-0.039641	2.135771
204.584831	1385.622183	18.409779	-0.039651	2.130504
204.541283	1377.700634	18.414784	-0.039638	2.125248
204.334208	1369.785660	18.419789	-0.039594	2.119967
204.435041	1361.870923	18.424794	-0.039608	2.114704
204.248045	1353.859132	18.429799	-0.039568	2.109334
203.877319	1345.959853	18.434803	-0.039494	2.104008
204.048698	1338.013229	18.439808	-0.039521	2.098690
203.814452	1330.095628	18.444813	-0.039473	2.093338
203.891663	1322.133333	18.449818	-0.039482	2.087972
203.955568	1314.196584	18.454823	-0.039489	2.082609
203.965441	1306.266703	18.459827	-0.039486	2.077231
203.878466	1298.360902	18.464832	-0.039465	2.071846
203.720543	1290.414949	18.469837	-0.039430	2.066412
203.807511	1282.483156	18.474842	-0.039442	2.060999
203.631848	1274.579395	18.479847	-0.039404	2.055564
203.515508	1266.631475	18.484851	-0.039377	2.050090
203.484446	1258.724231	18.489856	-0.039367	2.044638
203.465135	1250.790325	18.494861	-0.039358	2.039154
203.516580	1242.861714	18.499866	-0.039363	2.033666
203.394852	1234.896476	18.504871	-0.039335	2.028120
203.304440	1226.980923	18.509875	-0.039313	2.022597
203.196979	1219.078619	18.514880	-0.039288	2.017067
203.247210	1211.118864	18.519885	-0.039292	2.011497
203.386959	1203.174712	18.524890	-0.039314	2.005931
203.209214	1195.285604	18.529895	-0.039275	2.000356
203.084483	1187.396166	18.534899	-0.039247	1.994771
203.158668	1179.449145	18.539904	-0.039256	1.989150
203.158200	1171.509496	18.544909	-0.039251	1.983511
203.006651	1163.621045	18.549914	-0.039218	1.977876
202.801536	1155.718648	18.554919	-0.039175	1.972209
203.004268	1147.743997	18.559923	-0.039208	1.966518
202.909793	1139.855364	18.564928	-0.039185	1.960840
202.611951	1131.978561	18.569933	-0.039125	1.955132
202.675351	1123.995300	18.574938	-0.039131	1.949369
202.647832	1116.059968	18.579943	-0.039121	1.943614
202.398494	1108.179988	18.584947	-0.039070	1.937858
202.380869	1100.262197	18.589952	-0.039062	1.932083
202.374366	1092.325467	18.594957	-0.039056	1.926278
202.221156	1084.432444	18.599962	-0.039022	1.920471
202.119900	1076.538802	18.604967	-0.038998	1.914652
202.191507	1068.591097	18.609971	-0.039007	1.908794
202.076209	1060.701069	18.614976	-0.038980	1.902940
202.019475	1052.781792	18.619981	-0.038965	1.897053
201.965044	1044.874208	18.624986	-0.038950	1.891156
202.019918	1036.946721	18.629991	-0.038955	1.885239
201.917302	1029.063452	18.634995	-0.038931	1.879318
201.853068	1021.168967	18.640000	-0.038914	1.873374
201.808729	1013.226272	18.645005	-0.038901	1.867378
201.598847	1005.360963	18.650010	-0.038857	1.861401
201.669142	997.428706	18.655015	-0.038865	1.855387
201.681854	989.510842	18.660019	-0.038862	1.849357
201.615361	981.629271	18.665024	-0.038845	1.843327
201.403040	973.749776	18.670029	-0.038800	1.837260
201.425573	965.844321	18.675034	-0.038800	1.831182
201.252221	957.957466	18.680039	-0.038762	1.825074
201.161954	950.060568	18.685043	-0.038741	1.818948
201.239524	942.149156	18.690048	-0.038750	1.812810
201.106088	934.254273	18.695053	-0.038720	1.806639
201.439446	926.327738	18.700058	-0.038777	1.800478
201.031189	918.496463	18.705063	-0.038696	1.794280
200.999871	910.531226	18.710067	-0.038686	1.788002
200.959770	902.650308	18.715072	-0.038673	1.781767
200.641142	894.799040	18.720077	-0.038609	1.775499
200.625834	886.900518	18.725082	-0.038601	1.769209
200.595455	879.003733	18.730087	-0.038591	1.762896
200.411837	871.153306	18.735091	-0.038551	1.756578
200.409940	863.251726	18.740096	-0.038546	1.750220
200.478433	855.336544	18.745101	-0.038554	1.743835
200.457945	847.469363	18.750106	-0.038545	1.737455
200.572927	839.550429	18.755111	-0.038562	1.731027
200.231941	831.720917	18.760115	-0.038493	1.724589
200.452800	823.836744	18.765120	-0.038529	1.718155
200.239248	815.968431	18.770125	-0.038485	1.711653
200.184347	808.079316	18.775130	-0.038470	1.705130
200.083143	800.215668	18.780135	-0.038446	1.698597
199.983883	792.343075	18.785139	-0.038422	1.692032
199.999579	784.456042	18.790144	-0.038420	1.685443
199.893867	776.608045	18.795149	-0.038396	1.678846
199.927985	768.738429	18.800154	-0.038397	1.672223
199.745473	760.875145	18.805159	-0.038358	1.665550
199.769564	753.007534	18.810163	-0.038358	1.658875
199.742399	745.150601	18.815168	-0.038348	1.652174
199.479595	737.296798	18.820173	-0.038294	1.645417
199.410644	729.462481	18.825178	-0.038276	1.638675
199.521820	721.538128	18.830183	-0.038292	1.631853
199.361768	713.664938	18.835187	-0.038257	1.625008
199.429818	705.816421	18.840192	-0.038265	1.618188
199.465751	697.937375	18.845197	-0.038267	1.611308
199.385303	690.098125	18.850202	-0.038247	1.604416
199.159168	682.295477	18.855207	-0.038200	1.597507
199.036357	674.448728	18.860211	-0.038172	1.590543
199.065946	666.600644	18.865216	-0.038173	1.583570
198.973607	658.756630	18.870221	-0.038151	1.576551
199.101655	650.884560	18.875226	-0.038170	1.569508
199.050768	643.057340	18.880231	-0.038155	1.562447
198.930382	635.244032	18.885235	-0.038128	1.555357
198.617233	627.432893	18.890240	-0.038065	1.548208
198.668317	619.566298	18.895245	-0.038069	1.541029
198.803608	611.720677	18.900250	-0.038089	1.533848
198.645778	603.897570	18.905255	-0.038055	1.526610
198.445663	596.101226	18.910259	-0.038013	1.519356
198.393294	588.289580	18.915264	-0.037998	1.512075
198.316496	580.451599	18.920269	-0.037979	1.504731
198.326807	572.643616	18.925274	-0.037976	1.497392
198.128750	564.839145	18.930279	-0.037934	1.489988
198.208761	557.005122	18.935283	-0.037944	1.482562
198.168997	549.207428	18.940288	-0.037932	1.475115
198.064178	541.340088	18.945293	-0.037908	1.467553
198.058381	533.542274	18.950298	-0.037902	1.460035
197.938307	525.755443	18.955303	-0.037875	1.452470
197.746180	517.967221	18.960307	-0.037834	1.444852
197.862178	510.169728	18.965312	-0.037851	1.437235
197.582569	502.401749	18.970317	-0.037794	1.429542
197.514225	494.614497	18.975322	-0.037776	1.421823
197.700914	486.799637	18.980327	-0.037806	1.414076
197.396190	479.040482	18.985331	-0.037744	1.406261
197.299046	471.292950	18.990336	-0.037721	1.398448
197.299519	463.481609	18.995341	-0.037717	1.390543
197.246581	455.705079	19.000346	-0.037702	1.382619
197.267301	447.924778	19.005351	-0.037701	1.374659
197.134970	440.159542	19.010355	-0.037671	1.366641
197.027926	432.429841	19.015360	-0.037647	1.358617
197.046369	424.648829	19.020365	-0.037645	1.350514
196.993506	416.895972	19.025370	-0.037630	1.342379
197.006589	409.138129	19.030375	-0.037628	1.334200
197.065811	401.364152	19.035379	-0.037634	1.325962
196.902330	393.673834	19.040384	-0.037599	1.317723
196.734981	385.845948	19.045389	-0.037563	1.309282
196.722718	378.087882	19.050394	-0.037556	1.300891
196.661880	370.379175	19.055399	-0.037540	1.292490
196.407890	362.683370	19.060403	-0.037487	1.284012
196.550579	354.954437	19.065408	-0.037509	1.275516
196.325224	347.262213	19.070413	-0.037462	1.266934
196.114358	339.592053	19.075418	-0.037418	1.258321
196.186139	331.863984	19.080423	-0.037427	1.249637
196.016806	324.183903	19.085427	-0.037391	1.240901
195.912674	316.516872	19.090432	-0.037366	1.232130
195.768318	308.815091	19.095437	-0.037335	1.223248
195.842449	301.122747	19.100442	-0.037344	1.214355
195.609494	293.476115	19.105447	-0.037295	1.205389
195.556617	285.817105	19.110451	-0.037281	1.196378
195.486328	278.155270	19.115456	-0.037263	1.187291
195.448161	270.492874	19.120461	-0.037251	1.178139
195.541773	262.822400	19.125466	-0.037264	1.168934
195.267658	255.232366	19.130471	-0.037208	1.159677
195.230771	247.563374	19.135475	-0.037196	1.150298
195.002402	239.953895	19.140480	-0.037149	1.140875
194.819668	232.352353	19.145485	-0.037110	1.131393
194.845034	224.726736	19.150490	-0.037110	1.121846
194.696024	217.149488	19.155495	-0.037078	1.112240
194.652558	209.541230	19.160499	-0.037065	1.102534
194.651450	201.960602	19.165504	-0.037060	1.092786
194.457277	194.397711	19.170509	-0.037019	1.082931
194.512822	186.824764	19.175514	-0.037025	1.073028
194.356559	179.272589	19.180519	-0.036991	1.063013
194.298681	171.725214	19.185523	-0.036975	1.052931
194.357210	164.175459	19.190528	-0.036981	1.042775
194.115161	156.686694	19.195533	-0.036932	1.032532
193.959529	149.190321	19.200538	-0.036898	1.022197
193.804766	141.707441	19.205543	-0.036864	1.011774
193.641861	134.234010	19.210547	-0.036829	1.001255
193.594314	126.744078	19.215552	-0.036816	0.990629
193.377907	119.279663	19.220557	-0.036771	0.979882
193.203074	111.846076	19.225562	-0.036734	0.969071
193.372019	104.374077	19.230567	-0.036761	0.958170
192.951608	97.006179	19.235571	-0.036678	0.947145
192.886978	89.613896	19.240576	-0.036661	0.936047
192.531467	82.262895	19.245581	-0.036590	0.924801
192.394098	74.907812	19.250586	-0.036560	0.913469
192.499645	67.506298	19.255591	-0.036575	0.901989
192.040300	60.465024	19.260595	-0.036485	0.890774