Thu Mar 11 18:20:48 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.388850	0.068840	0.000000	0.000023	0.723794

0.520660	-0.007966	0.005005	-0.000002	0.723690
0.518331	-0.034202	0.010010	-0.000002	0.723638
0.517907	-0.039590	0.015014	-0.000002	0.723628
0.661400	-0.059968	0.020019	-0.000029	0.723638
0.502119	-0.035400	0.025024	0.000001	0.723631
0.518990	-0.038372	0.030029	-0.000002	0.723632
0.480188	-0.028484	0.035034	0.000005	0.723638
0.439562	-0.026237	0.040038	0.000012	0.723628
0.514841	-0.034470	0.045043	-0.000002	0.723639
0.398136	-0.016566	0.050048	0.000019	0.723633
0.343254	-0.006644	0.055053	0.000029	0.723634
0.157850	0.028390	0.060058	0.000064	0.723638
0.107621	0.032745	0.065062	0.000073	0.723630
0.291934	0.003307	0.070067	0.000038	0.723637
0.325182	-0.008036	0.075072	0.000032	0.723626
0.405510	-0.092506	0.080077	0.000017	0.723489
0.353017	-0.156938	0.085082	0.000027	0.723345
0.229297	-0.140849	0.090086	0.000049	0.723334
0.292076	-0.148213	0.095091	0.000038	0.723341
0.350012	-0.160128	0.100096	0.000027	0.723339
0.238538	-0.139652	0.105101	0.000047	0.723340
0.393513	-0.163828	0.110106	0.000018	0.723347
0.396545	-0.298781	0.115110	0.000018	0.723084
0.573210	-0.369279	0.120115	-0.000015	0.723008
0.460331	-0.351536	0.125120	0.000005	0.723003
0.379081	-0.336282	0.130125	0.000020	0.723005
0.568135	-0.367324	0.135130	-0.000015	0.723011
0.228374	-0.458083	0.140134	0.000048	0.722714
0.126546	-0.449426	0.145139	0.000067	0.722696
0.144438	-0.455881	0.150144	0.000063	0.722690
0.430792	-0.507352	0.155149	0.000010	0.722689
0.360599	-0.580201	0.160154	0.000023	0.722522
0.152565	-0.623597	0.165158	0.000061	0.722364
0.153797	-0.619570	0.170163	0.000061	0.722373
0.171871	-0.624386	0.175168	0.000057	0.722370
0.192588	-0.732501	0.180173	0.000054	0.722166
0.303190	-0.797069	0.185178	0.000033	0.722078
0.284700	-0.799109	0.190182	0.000036	0.722068
0.227356	-0.829476	0.195187	0.000047	0.721988
0.157130	-0.942631	0.200192	0.000060	0.721742
0.159685	-0.944127	0.205197	0.000059	0.721740
0.140553	-0.950658	0.210202	0.000062	0.721721
-0.003545	-1.072210	0.215206	0.000089	0.721432
0.032569	-1.075275	0.220211	0.000082	0.721439
-0.113570	-1.056525	0.225216	0.000109	0.721425
-0.091090	-1.214346	0.230221	0.000105	0.721123
-0.057727	-1.219025	0.235226	0.000099	0.721125
-0.134588	-1.228204	0.240230	0.000113	0.721081
-0.249514	-1.308764	0.245235	0.000134	0.720882
-0.383810	-1.288666	0.250240	0.000159	0.720875
-0.281623	-1.365658	0.255245	0.000140	0.720760
-0.237852	-1.483871	0.260250	0.000131	0.720543
-0.436024	-1.453902	0.265254	0.000168	0.720533
-0.245638	-1.593233	0.270259	0.000133	0.720325
-0.246196	-1.645464	0.275264	0.000132	0.720223
-0.452011	-1.641715	0.280269	0.000171	0.720158
-0.392501	-1.782685	0.285274	0.000159	0.719902
-0.573639	-1.754040	0.290278	0.000193	0.719895
-0.729431	-1.834718	0.295283	0.000222	0.719682
-1.317548	-1.771214	0.300288	0.000331	0.719601
-1.844349	-1.692292	0.305293	0.000429	0.719572
-2.508588	-1.725273	0.310298	0.000553	0.719274
-2.906827	-1.657721	0.315302	0.000627	0.719267
-3.043549	-1.630056	0.320307	0.000652	0.719274
-3.242996	-1.717774	0.325312	0.000689	0.719032
-4.076310	-1.604543	0.330317	0.000844	0.718963
-3.875069	-1.637860	0.335322	0.000806	0.718968
-4.197659	-1.586864	0.340326	0.000866	0.718955
-4.616913	-1.663018	0.345331	0.000944	0.718658
-4.859845	-1.627313	0.350336	0.000989	0.718644
-5.189298	-1.569989	0.355341	0.001050	0.718641
-4.882910	-1.621285	0.360346	0.000993	0.718648
-5.049947	-1.674813	0.365350	0.001024	0.718484
-5.682409	-1.625939	0.370355	0.001141	0.718358
-5.548858	-1.653095	0.375360	0.001116	0.718352
-6.103787	-1.555334	0.380365	0.001219	0.718350
-5.654973	-1.630616	0.385370	0.001136	0.718360
-6.422732	-1.663370	0.390374	0.001279	0.718025
-6.794155	-1.602834	0.395379	0.001348	0.718015
-6.677439	-1.624540	0.400384	0.001326	0.718013
-6.473244	-1.662578	0.405389	0.001287	0.718010
-6.768854	-1.603654	0.410394	0.001342	0.718023
-7.260352	-1.643865	0.415398	0.001434	0.717771
-7.497672	-1.635013	0.420403	0.001478	0.717705
-7.727041	-1.596142	0.425408	0.001520	0.717701
-7.949190	-1.557215	0.430413	0.001561	0.717700
-7.491795	-1.636482	0.435418	0.001476	0.717705
-7.781785	-1.588709	0.440422	0.001530	0.717698
-7.953698	-1.705163	0.445427	0.001562	0.717407
-8.544347	-1.615162	0.450432	0.001671	0.717378
-8.771645	-1.576737	0.455437	0.001714	0.717374
-8.475527	-1.623334	0.460442	0.001658	0.717386
-8.760262	-1.579967	0.465446	0.001711	0.717372
-8.584231	-1.608726	0.470451	0.001678	0.717378
-8.840053	-1.682506	0.475456	0.001726	0.717142
-9.621834	-1.575181	0.480461	0.001871	0.717079
-8.984186	-1.685890	0.485466	0.001752	0.717085
-9.172246	-1.657491	0.490470	0.001787	0.717075
-9.553405	-1.585937	0.495475	0.001858	0.717083
-9.321859	-1.628690	0.500480	0.001815	0.717080
-9.701518	-1.677756	0.505485	0.001885	0.716850
-10.500781	-1.583271	0.510490	0.002034	0.716755
-10.328406	-1.621005	0.515494	0.002001	0.716742
-10.193702	-1.638620	0.520499	0.001976	0.716755
-10.625695	-1.562507	0.525504	0.002056	0.716753
-10.680654	-1.555684	0.530509	0.002066	0.716748
-10.029960	-1.668130	0.535514	0.001945	0.716755
-10.835964	-1.672455	0.540518	0.002095	0.716463
-11.482631	-1.565707	0.545523	0.002215	0.716446
-11.264479	-1.605877	0.550528	0.002174	0.716444
-11.011251	-1.652256	0.555533	0.002127	0.716442
-11.067415	-1.638201	0.560538	0.002137	0.716450
-11.479589	-1.570425	0.565542	0.002214	0.716439
-11.376808	-1.596547	0.570547	0.002195	0.716424
-11.667115	-1.693999	0.575552	0.002249	0.716129
-12.512876	-1.546500	0.580557	0.002406	0.716123
-12.377925	-1.565506	0.585562	0.002381	0.716133
-12.111789	-1.618006	0.590566	0.002331	0.716124
-12.365624	-1.570907	0.595571	0.002378	0.716128
-12.475333	-1.551373	0.600576	0.002398	0.716128
-12.331229	-1.578905	0.605581	0.002371	0.716125
-12.329523	-1.664032	0.610586	0.002371	0.715957
-13.417479	-1.508754	0.615590	0.002573	0.715881
-12.951103	-1.591095	0.620595	0.002486	0.715883
-12.700294	-1.636177	0.625600	0.002439	0.715882
-13.611617	-1.477192	0.630605	0.002609	0.715876
-12.866531	-1.605086	0.635610	0.002470	0.715886
-12.957787	-1.594077	0.640614	0.002487	0.715876
-13.616916	-1.616256	0.645619	0.002609	0.715599
-14.029442	-1.570372	0.650624	0.002686	0.715545
-13.847484	-1.606615	0.655629	0.002652	0.715538
-13.699664	-1.627958	0.660634	0.002624	0.715548
-14.228715	-1.539665	0.665638	0.002722	0.715536
-14.143698	-1.550411	0.670643	0.002706	0.715545
-13.919696	-1.590719	0.675648	0.002665	0.715545
-14.512103	-1.604015	0.680653	0.002775	0.715310
-15.165369	-1.524439	0.685658	0.002896	0.715237
-14.694638	-1.613541	0.690662	0.002808	0.715227
-14.948638	-1.568498	0.695667	0.002855	0.715227
-15.090722	-1.542409	0.700672	0.002882	0.715229
-15.037900	-1.552969	0.705677	0.002872	0.715227
-14.782404	-1.593498	0.710682	0.002824	0.715237
-15.019529	-1.615866	0.715686	0.002868	0.715109
-15.953865	-1.550078	0.720691	0.003042	0.714910
-15.433537	-1.644909	0.725696	0.002945	0.714906
-16.250435	-1.501510	0.730701	0.003097	0.714902
-15.868944	-1.565708	0.735706	0.003025	0.714910
-15.526991	-1.632143	0.740710	0.002962	0.714899
-15.989320	-1.546288	0.745715	0.003047	0.714906
-15.830581	-1.605291	0.750720	0.003018	0.714846
-16.406722	-1.626036	0.755725	0.003125	0.714601
-16.216203	-1.654878	0.760730	0.003089	0.714612
-17.017450	-1.516505	0.765734	0.003238	0.714603
-16.821954	-1.548749	0.770739	0.003202	0.714609
-16.454425	-1.615061	0.775744	0.003133	0.714607
-16.821581	-1.552962	0.780749	0.003201	0.714601
-16.532094	-1.653719	0.785754	0.003147	0.714504
-17.421435	-1.612237	0.790758	0.003313	0.714272
-17.262277	-1.636673	0.795763	0.003283	0.714280
-17.743046	-1.552758	0.800768	0.003372	0.714277
-17.699008	-1.563011	0.805773	0.003364	0.714272
-17.493355	-1.594709	0.810778	0.003325	0.714283
-17.932462	-1.522028	0.815782	0.003407	0.714272
-17.697975	-1.581927	0.820787	0.003363	0.714236
-18.091107	-1.646749	0.825792	0.003436	0.713969
-18.674776	-1.545205	0.830797	0.003544	0.713964
-18.903229	-1.502157	0.835802	0.003587	0.713969
-18.491867	-1.579816	0.840806	0.003510	0.713961
-18.639351	-1.550133	0.845811	0.003537	0.713968
-18.866277	-1.509281	0.850816	0.003579	0.713969
-18.663834	-1.547558	0.855821	0.003542	0.713965
-18.378108	-1.683726	0.860826	0.003488	0.713796
-19.910176	-1.488428	0.865830	0.003773	0.713642
-19.610640	-1.537566	0.870835	0.003717	0.713650
-19.266735	-1.600340	0.875840	0.003653	0.713648
-19.535723	-1.554742	0.880845	0.003703	0.713643
-19.601844	-1.538457	0.885850	0.003715	0.713653
-19.497994	-1.561013	0.890854	0.003696	0.713645
-19.372047	-1.618829	0.895859	0.003672	0.713575
-20.385252	-1.549615	0.900864	0.003861	0.713354
-20.449295	-1.541902	0.905869	0.003872	0.713347
-20.323205	-1.559198	0.910874	0.003849	0.713358
-20.612860	-1.510190	0.915878	0.003902	0.713353
-20.575490	-1.515250	0.920883	0.003895	0.713356
-20.169007	-1.587448	0.925888	0.003819	0.713357
-20.266026	-1.573782	0.930893	0.003837	0.713350
-20.831189	-1.624638	0.935898	0.003942	0.713049
-21.341534	-1.552504	0.940902	0.004037	0.713012
-21.335049	-1.551983	0.945907	0.004036	0.713016
-21.169807	-1.578337	0.950912	0.004005	0.713022
-21.453658	-1.531184	0.955917	0.004058	0.713016
-20.880514	-1.629588	0.960922	0.003951	0.713023
-21.161481	-1.585067	0.965926	0.004003	0.713013
-22.127516	-1.551286	0.970931	0.004182	0.712738
-21.969926	-1.594900	0.975936	0.004153	0.712707
-22.310026	-1.537996	0.980941	0.004216	0.712700
-22.239304	-1.545551	0.985946	0.004203	0.712710
-22.209913	-1.555110	0.990950	0.004197	0.712702
-22.320933	-1.532595	0.995955	0.004218	0.712708
-22.359131	-1.525289	1.000960	0.004225	0.712709
-22.495284	-1.553565	1.005965	0.004250	0.712605
-22.895211	-1.591260	1.010970	0.004324	0.712388
-22.914560	-1.593700	1.015974	0.004327	0.712377
-23.320079	-1.515106	1.020979	0.004403	0.712390
-22.917684	-1.586973	1.025984	0.004328	0.712390
-22.928287	-1.588425	1.030989	0.004330	0.712383
-23.358778	-1.507301	1.035994	0.004409	0.712393
-23.478894	-1.506440	1.040998	0.004432	0.712352
-23.736641	-1.592378	1.046003	0.004480	0.712090
-23.941806	-1.554578	1.051008	0.004518	0.712092
-24.269319	-1.500146	1.056013	0.004578	0.712085
-23.663689	-1.604194	1.061018	0.004465	0.712093
-23.919384	-1.562677	1.066022	0.004513	0.712085
-24.424279	-1.472017	1.071027	0.004607	0.712087
-23.739035	-1.593150	1.076032	0.004479	0.712089
-24.479730	-1.629155	1.081037	0.004617	0.711755
-25.010950	-1.531062	1.086042	0.004715	0.711762
-24.978939	-1.541630	1.091046	0.004709	0.711752
-24.510915	-1.621515	1.096051	0.004622	0.711760
-24.774733	-1.572950	1.101056	0.004671	0.711763
-25.457634	-1.454719	1.106061	0.004798	0.711757
-24.604738	-1.602754	1.111066	0.004639	0.711765
-25.090482	-1.659651	1.116070	0.004729	0.711479
-26.097366	-1.494444	1.121075	0.004916	0.711451
-25.962160	-1.517882	1.126080	0.004891	0.711453
-25.740922	-1.560212	1.131085	0.004850	0.711447
-25.917373	-1.523498	1.136090	0.004882	0.711458
-26.010136	-1.512065	1.141094	0.004899	0.711448
-25.686037	-1.570102	1.146099	0.004839	0.711448
-25.643103	-1.671854	1.151104	0.004831	0.711261
-27.151454	-1.467735	1.156109	0.005111	0.711132
-26.377293	-1.601789	1.161114	0.004967	0.711140
-26.490752	-1.585179	1.166118	0.004988	0.711133
-27.016956	-1.490639	1.171123	0.005086	0.711135
-26.535244	-1.575004	1.176128	0.004996	0.711138
-26.627084	-1.562716	1.181133	0.005013	0.711131
-26.716811	-1.630071	1.186138	0.005030	0.710965
-27.638092	-1.516969	1.191142	0.005201	0.710863
-27.236585	-1.586652	1.196147	0.005126	0.710867
-27.273747	-1.580627	1.201152	0.005133	0.710866
-27.874530	-1.476275	1.206157	0.005244	0.710861
-27.289813	-1.575479	1.211162	0.005135	0.710871
-27.268993	-1.584008	1.216166	0.005131	0.710862
-28.033782	-1.593366	1.221171	0.005274	0.710572
-28.451502	-1.539920	1.226176	0.005351	0.710530
-28.219588	-1.584151	1.231181	0.005308	0.710524
-27.848805	-1.647346	1.236186	0.005239	0.710531
-28.508111	-1.532131	1.241190	0.005361	0.710526
-28.590553	-1.516590	1.246195	0.005376	0.710528
-28.129031	-1.598026	1.251200	0.005290	0.710530
-29.212398	-1.564362	1.256205	0.005492	0.710212
-29.335328	-1.539107	1.261210	0.005514	0.710219
-29.395739	-1.532687	1.266214	0.005526	0.710211
-29.401446	-1.530392	1.271219	0.005526	0.710214
-29.351623	-1.537212	1.276224	0.005517	0.710218
-29.352662	-1.541100	1.281229	0.005517	0.710210
-28.998742	-1.602073	1.286234	0.005451	0.710215
-29.727598	-1.578491	1.291238	0.005586	0.710003
-30.607744	-1.477790	1.296243	0.005750	0.709891
-30.059615	-1.573533	1.301248	0.005648	0.709895
-30.504431	-1.500674	1.306253	0.005731	0.709883
-30.534835	-1.488395	1.311258	0.005736	0.709897
-30.133997	-1.564604	1.316262	0.005661	0.709887
-30.225403	-1.547037	1.321267	0.005678	0.709890
-30.490717	-1.507924	1.326272	0.005727	0.709874
-30.860737	-1.584604	1.331277	0.005796	0.709589
-30.789956	-1.594186	1.336282	0.005783	0.709596
-31.399720	-1.489272	1.341286	0.005896	0.709589
-31.129518	-1.535916	1.346291	0.005846	0.709592
-30.613572	-1.625770	1.351296	0.005749	0.709597
-31.307021	-1.506723	1.356301	0.005878	0.709588
-31.131456	-1.558352	1.361306	0.005845	0.709547
-31.806807	-1.581755	1.366310	0.005971	0.709260
-32.013904	-1.544935	1.371315	0.006009	0.709260
-32.082628	-1.530357	1.376320	0.006022	0.709265
-32.347856	-1.487896	1.381325	0.006071	0.709256
-31.823531	-1.577258	1.386330	0.005973	0.709265
-32.136102	-1.525541	1.391334	0.006031	0.709257
-32.055794	-1.538070	1.396339	0.006016	0.709261
-32.150747	-1.653233	1.401344	0.006034	0.708997
-33.255046	-1.480445	1.406349	0.006239	0.708949
-33.142482	-1.495489	1.411354	0.006218	0.708959
-32.663388	-1.583304	1.416358	0.006129	0.708955
-33.017554	-1.520935	1.421363	0.006194	0.708954
-33.279625	-1.471782	1.426368	0.006243	0.708959
-33.195770	-1.490910	1.431373	0.006227	0.708951
-32.730718	-1.653558	1.436378	0.006141	0.708791
-34.124142	-1.481525	1.441382	0.006400	0.708639
-33.856352	-1.531525	1.446387	0.006350	0.708635
-33.478987	-1.595832	1.451392	0.006279	0.708641
-33.951487	-1.517514	1.456397	0.006367	0.708629
-33.711216	-1.555828	1.461402	0.006322	0.708639
-33.667755	-1.565885	1.466406	0.006314	0.708635
-33.865984	-1.625240	1.471411	0.006351	0.708445
-34.703905	-1.523623	1.476416	0.006507	0.708350
-34.726639	-1.524646	1.481421	0.006511	0.708340
-34.253003	-1.603349	1.486426	0.006422	0.708352
-34.748682	-1.518324	1.491430	0.006514	0.708346
-34.862249	-1.499691	1.496435	0.006535	0.708343
-34.268527	-1.602602	1.501440	0.006425	0.708349
-34.882300	-1.639871	1.506445	0.006539	0.708055
-35.527239	-1.545136	1.511450	0.006659	0.708015
-35.450697	-1.563423	1.516454	0.006644	0.708006
-35.183102	-1.610117	1.521459	0.006594	0.708008
-35.502981	-1.550233	1.526464	0.006654	0.708014
-35.781108	-1.505889	1.531469	0.006705	0.708004
-35.182336	-1.622940	1.536474	0.006594	0.707984
-36.110283	-1.602844	1.541478	0.006766	0.707693
-36.472966	-1.538600	1.546483	0.006834	0.707692
-36.570602	-1.520664	1.551488	0.006852	0.707694
-36.380281	-1.556466	1.556493	0.006816	0.707690
-36.505359	-1.530370	1.561498	0.006839	0.707698
-36.547115	-1.524301	1.566502	0.006847	0.707696
-36.236872	-1.579571	1.571507	0.006789	0.707696
-36.548582	-1.663261	1.576512	0.006847	0.707417
-37.595810	-1.499323	1.581517	0.007041	0.707372
-37.354455	-1.539555	1.586522	0.006996	0.707378
-37.204427	-1.569692	1.591526	0.006968	0.707371
-37.595131	-1.499440	1.596531	0.007041	0.707373
-37.413225	-1.530864	1.601536	0.007007	0.707375
-37.325350	-1.550467	1.606541	0.006990	0.707368
-37.738106	-1.563627	1.611546	0.007067	0.707194
-38.461515	-1.494255	1.616550	0.007201	0.707075
-38.021284	-1.571455	1.621555	0.007119	0.707078
-37.958194	-1.581507	1.626560	0.007107	0.707080
-38.659512	-1.460436	1.631565	0.007238	0.707073
-37.912258	-1.589446	1.636570	0.007098	0.707082
-38.067562	-1.564418	1.641574	0.007127	0.707077
-38.729838	-1.529447	1.646579	0.007250	0.706910
-39.338135	-1.500462	1.651584	0.007363	0.706751
-39.156328	-1.536223	1.656589	0.007329	0.706745
-39.111773	-1.541573	1.661594	0.007321	0.706750
-39.457118	-1.483368	1.666598	0.007385	0.706744
-39.069525	-1.550760	1.671603	0.007313	0.706747
-39.023639	-1.557396	1.676608	0.007304	0.706751
-39.433493	-1.488119	1.681613	0.007380	0.706744
-39.512274	-1.612041	1.686618	0.007395	0.706467
-39.887378	-1.560141	1.691622	0.007464	0.706437
-40.470791	-1.455845	1.696627	0.007573	0.706438
-39.840825	-1.564968	1.701632	0.007455	0.706445
-39.909761	-1.556109	1.706637	0.007468	0.706438
-40.142316	-1.511015	1.711642	0.007511	0.706446
-40.230919	-1.498107	1.716646	0.007527	0.706440
-40.401532	-1.599423	1.721651	0.007559	0.706176
-40.645829	-1.579841	1.726656	0.007604	0.706128
-41.080804	-1.505729	1.731661	0.007685	0.706121
-40.710605	-1.568977	1.736666	0.007616	0.706127
-40.817042	-1.550598	1.741670	0.007636	0.706126
-40.946556	-1.528609	1.746675	0.007660	0.706125
-40.683121	-1.579463	1.751680	0.007610	0.706117
-41.261288	-1.607134	1.756685	0.007718	0.705855
-41.428683	-1.573541	1.761690	0.007749	0.705862
-41.783858	-1.511751	1.766694	0.007815	0.705860
-41.701198	-1.529215	1.771699	0.007799	0.705855
-41.532548	-1.555876	1.776704	0.007768	0.705862
-42.154696	-1.448590	1.781709	0.007883	0.705855
-41.578172	-1.598638	1.786714	0.007776	0.705760
-42.459821	-1.561508	1.791718	0.007940	0.705519
-42.632483	-1.530391	1.796723	0.007972	0.705520
-42.733566	-1.509125	1.801728	0.007990	0.705527
-42.605741	-1.537471	1.806733	0.007966	0.705516
-42.640209	-1.527304	1.811738	0.007973	0.705524
-42.778322	-1.504363	1.816742	0.007998	0.705521
-42.603301	-1.557024	1.821747	0.007965	0.705478
-43.189701	-1.583680	1.826752	0.008074	0.705215
-43.686899	-1.499824	1.831757	0.008167	0.705205
-43.779928	-1.479840	1.836762	0.008184	0.705213
-43.272071	-1.572482	1.841766	0.008089	0.705209
-43.440765	-1.544863	1.846771	0.008120	0.705204
-43.562747	-1.520880	1.851776	0.008143	0.705209
-43.271398	-1.598147	1.856781	0.008089	0.705158
-44.029887	-1.597896	1.861786	0.008230	0.704887
-44.268171	-1.556784	1.866790	0.008274	0.704884
-44.341161	-1.545488	1.871795	0.008287	0.704881
-43.994186	-1.602127	1.876800	0.008222	0.704892
-44.581789	-1.502266	1.881805	0.008332	0.704883
-44.441366	-1.524948	1.886810	0.008305	0.704888
-44.133707	-1.637154	1.891814	0.008248	0.704772
-45.505930	-1.486584	1.896819	0.008503	0.704583
-45.164575	-1.543309	1.901824	0.008440	0.704592
-45.403976	-1.504901	1.906829	0.008484	0.704584
-45.336583	-1.513946	1.911834	0.008471	0.704590
-45.263169	-1.529138	1.916838	0.008457	0.704586
-45.486968	-1.491846	1.921843	0.008499	0.704581
-45.148141	-1.571979	1.926848	0.008436	0.704542
-46.275121	-1.516045	1.931853	0.008645	0.704250
-46.212811	-1.523062	1.936858	0.008633	0.704258
-46.287101	-1.512695	1.941862	0.008647	0.704253
-46.317246	-1.507991	1.946867	0.008653	0.704252
-46.211340	-1.524097	1.951872	0.008633	0.704258
-46.395320	-1.495567	1.956877	0.008667	0.704250
-46.194807	-1.526914	1.961882	0.008629	0.704259
-46.493156	-1.569616	1.966886	0.008685	0.704066
-47.578368	-1.436365	1.971891	0.008886	0.703945
-46.634062	-1.600401	1.976896	0.008711	0.703954
-46.992558	-1.543154	1.981901	0.008777	0.703941
-47.375565	-1.471205	1.986906	0.008848	0.703948
-46.917462	-1.553549	1.991910	0.008763	0.703947
-47.117408	-1.520158	1.996915	0.008800	0.703943
-47.788343	-1.517806	2.001920	0.008925	0.703707

-48.014233	-1.515665	2.011917	0.008966	0.703631
-47.805662	-1.552837	2.021914	0.008927	0.703631
-48.138310	-1.495063	2.031910	0.008989	0.703629
-47.789532	-1.556923	2.041907	0.008923	0.703630
-48.031423	-1.514555	2.051904	0.008968	0.703629
-47.774893	-1.560239	2.061901	0.008920	0.703630
-47.967205	-1.526595	2.071898	0.008955	0.703629
-48.226601	-1.480178	2.081894	0.009003	0.703630
-47.967370	-1.526653	2.091891	0.008955	0.703631
-48.056489	-1.511911	2.101888	0.008971	0.703629
-47.888026	-1.524504	2.111885	0.008939	0.703665
-47.204191	-1.507692	2.121882	0.008812	0.703945
-46.966312	-1.552219	2.131878	0.008767	0.703942
-47.075976	-1.532265	2.141875	0.008787	0.703943
-47.066040	-1.533441	2.151872	0.008785	0.703945
-46.817871	-1.578097	2.161869	0.008738	0.703945
-47.048569	-1.511185	2.171866	0.008781	0.703998
-46.236761	-1.529251	2.181862	0.008629	0.704254
-46.202217	-1.535743	2.191859	0.008623	0.704254
-46.408983	-1.499291	2.201856	0.008661	0.704254
-46.278086	-1.522846	2.211853	0.008636	0.704254
-45.552846	-1.498785	2.221850	0.008501	0.704564
-45.370664	-1.521709	2.231846	0.008466	0.704584
-45.305728	-1.532922	2.241843	0.008454	0.704585
-45.362164	-1.522224	2.251840	0.008464	0.704587
-44.407633	-1.551106	2.261837	0.008286	0.704872
-44.643632	-1.502073	2.271834	0.008330	0.704887
-44.474831	-1.532888	2.281830	0.008298	0.704886
-44.640515	-1.471130	2.291827	0.008328	0.704952
-43.784502	-1.494907	2.301824	0.008169	0.705212
-43.520056	-1.541530	2.311821	0.008119	0.705214
-43.720357	-1.506699	2.321818	0.008156	0.705212
-43.096153	-1.517950	2.331814	0.008039	0.705414
-42.693043	-1.536284	2.341811	0.007964	0.705523
-42.880609	-1.502249	2.351808	0.007999	0.705525
-42.601290	-1.552649	2.361805	0.007946	0.705524
-42.038330	-1.495704	2.371802	0.007841	0.705841
-41.744268	-1.539639	2.381798	0.007786	0.705859
-41.860445	-1.520351	2.391795	0.007807	0.705857
-41.650857	-1.526533	2.401792	0.007768	0.705920
-40.760763	-1.583788	2.411789	0.007602	0.706125
-41.302133	-1.487422	2.421786	0.007702	0.706125
-41.115188	-1.522208	2.431782	0.007667	0.706123
-40.584185	-1.479607	2.441779	0.007568	0.706400
-39.969440	-1.569029	2.451776	0.007453	0.706441
-40.138723	-1.537476	2.461773	0.007484	0.706444
-40.155986	-1.470209	2.471770	0.007487	0.706574
-39.306705	-1.536270	2.481766	0.007329	0.706746
-39.578798	-1.488685	2.491763	0.007379	0.706745
-39.250430	-1.528254	2.501760	0.007317	0.706784
-38.529964	-1.508969	2.511757	0.007183	0.707081
-38.484674	-1.518583	2.521754	0.007174	0.707078
-38.406212	-1.534303	2.531750	0.007159	0.707076
-38.269105	-1.464980	2.541747	0.007133	0.707264
-37.552234	-1.539863	2.551744	0.006999	0.707371
-37.464974	-1.554854	2.561741	0.006983	0.707373
-37.552312	-1.515047	2.571738	0.006999	0.707422
-36.665183	-1.538336	2.581734	0.006833	0.707694
-36.819537	-1.511508	2.591731	0.006862	0.707693
-36.674781	-1.535696	2.601728	0.006834	0.707697
-36.238572	-1.506423	2.611725	0.006753	0.707912
-35.956898	-1.507228	2.621722	0.006700	0.708012
-35.935828	-1.512759	2.631718	0.006696	0.708009
-35.971914	-1.458089	2.641715	0.006702	0.708106
-34.604080	-1.582669	2.651712	0.006447	0.708346
-34.893272	-1.530640	2.661709	0.006500	0.708348
-34.849017	-1.540460	2.671706	0.006492	0.708344
-34.484486	-1.509697	2.681702	0.006424	0.708537
-34.093497	-1.530249	2.691699	0.006351	0.708636
-33.949515	-1.556049	2.701696	0.006323	0.708636
-34.060913	-1.516435	2.711693	0.006344	0.708677
-32.998333	-1.566826	2.721690	0.006146	0.708956
-33.212647	-1.528495	2.731686	0.006185	0.708956
-33.032872	-1.563836	2.741683	0.006151	0.708951
-32.769200	-1.549366	2.751680	0.006102	0.709074
-32.214920	-1.553368	2.761677	0.005998	0.709265
-32.268506	-1.545713	2.771674	0.006008	0.709261
-32.526117	-1.501463	2.781670	0.006056	0.709259
-31.639210	-1.497133	2.791667	0.005890	0.709584
-31.408800	-1.534545	2.801664	0.005847	0.709592
-31.483949	-1.521955	2.811661	0.005860	0.709591
-31.013242	-1.517122	2.821658	0.005772	0.709770
-30.713241	-1.511473	2.831654	0.005716	0.709888
-30.492109	-1.551176	2.841651	0.005675	0.709888
-30.581643	-1.513234	2.851648	0.005691	0.709933
-29.706250	-1.528114	2.861645	0.005528	0.710216
-29.483436	-1.568742	2.871642	0.005486	0.710215
-29.859228	-1.503787	2.881638	0.005555	0.710211
-29.179370	-1.533091	2.891635	0.005429	0.710396
-28.546744	-1.580322	2.901632	0.005310	0.710527
-28.744499	-1.545062	2.911629	0.005347	0.710528
-28.792324	-1.536365	2.921626	0.005355	0.710529
-28.155009	-1.488216	2.931622	0.005236	0.710852
-27.867237	-1.534782	2.941619	0.005182	0.710862
-27.716485	-1.562254	2.951616	0.005154	0.710862
-27.764066	-1.494056	2.961613	0.005163	0.710982
-26.762676	-1.596444	2.971610	0.004976	0.711134
-27.220507	-1.516250	2.981606	0.005061	0.711132
-27.232481	-1.504268	2.991603	0.005063	0.711152
-26.512685	-1.485473	3.001600	0.004928	0.711447
-26.211091	-1.536964	3.011597	0.004872	0.711452
-26.471316	-1.490888	3.021594	0.004920	0.711452
-25.842790	-1.472301	3.031590	0.004802	0.711713
-25.488840	-1.514423	3.041587	0.004736	0.711755
-25.552277	-1.503766	3.051584	0.004748	0.711755
-25.119937	-1.485645	3.061581	0.004667	0.711945
-24.628405	-1.501494	3.071578	0.004575	0.712089
-24.709422	-1.487706	3.081574	0.004590	0.712088
-24.539494	-1.485650	3.091571	0.004558	0.712153
-23.734451	-1.512931	3.101568	0.004407	0.712385
-23.571002	-1.542859	3.111565	0.004377	0.712384
-23.709128	-1.517640	3.121562	0.004402	0.712386
-23.237402	-1.484310	3.131558	0.004314	0.712621
-22.815419	-1.517719	3.141555	0.004235	0.712705
-22.849965	-1.510327	3.151552	0.004241	0.712708
-22.544275	-1.531371	3.161549	0.004184	0.712775
-21.853724	-1.531463	3.171546	0.004055	0.713020
-21.763158	-1.548130	3.181542	0.004038	0.713020
-21.994062	-1.509050	3.191539	0.004080	0.713016
-21.547690	-1.490887	3.201536	0.003997	0.713212
-20.942909	-1.526300	3.211533	0.003884	0.713356
-21.126013	-1.495189	3.221530	0.003917	0.713354
-21.118135	-1.473706	3.231526	0.003916	0.713400
-20.066811	-1.537526	3.241523	0.003720	0.713646
-20.152800	-1.521753	3.251520	0.003735	0.713648
-20.010024	-1.545992	3.261517	0.003708	0.713651
-19.828335	-1.478925	3.271514	0.003674	0.713849
-19.117477	-1.547714	3.281510	0.003541	0.713965
-19.266398	-1.522263	3.291507	0.003569	0.713963
-19.104756	-1.548957	3.301504	0.003538	0.713968
-18.285858	-1.539390	3.311501	0.003386	0.714278
-18.440905	-1.511904	3.321498	0.003414	0.714278
-18.319965	-1.534217	3.331494	0.003391	0.714277
-18.211952	-1.478605	3.341491	0.003371	0.714427
-17.383394	-1.533476	3.351488	0.003216	0.714611
-17.395532	-1.532238	3.361485	0.003218	0.714610
-17.544531	-1.505082	3.371482	0.003245	0.714612
-16.814582	-1.496960	3.381478	0.003109	0.714887
-16.829107	-1.485649	3.391475	0.003111	0.714905
-16.561430	-1.533276	3.401472	0.003061	0.714906
-16.181440	-1.515096	3.411469	0.002990	0.715077
-15.671271	-1.528043	3.421466	0.002895	0.715232
-15.630837	-1.537747	3.431462	0.002887	0.715228
-15.937570	-1.482925	3.441459	0.002944	0.715229
-14.959848	-1.498277	3.451456	0.002761	0.715545
-14.811620	-1.524110	3.461453	0.002733	0.715546
-14.798917	-1.526234	3.471450	0.002731	0.715547
-14.583537	-1.497569	3.481446	0.002690	0.715681
-13.555382	-1.582015	3.491443	0.002498	0.715877
-13.690721	-1.556110	3.501440	0.002523	0.715881
-13.716126	-1.552746	3.511437	0.002528	0.715880
-13.359966	-1.552676	3.521434	0.002461	0.716006
-12.563716	-1.634184	3.531430	0.002312	0.716126
-12.919944	-1.570785	3.541427	0.002378	0.716127
-12.649824	-1.618132	3.551424	0.002328	0.716129
-12.152227	-1.604720	3.561421	0.002235	0.716332
-11.890801	-1.594597	3.571418	0.002186	0.716445
-11.878599	-1.599156	3.581414	0.002183	0.716441
-12.006892	-1.575492	3.591411	0.002207	0.716443
-11.023894	-1.601750	3.601408	0.002023	0.716738
-11.097817	-1.582006	3.611405	0.002037	0.716752
-10.986171	-1.602187	3.621402	0.002016	0.716752
-10.863048	-1.569248	3.631398	0.001992	0.716861
-10.070533	-1.599327	3.641395	0.001844	0.717082
-9.988603	-1.613543	3.651392	0.001829	0.717083
-10.241416	-1.567225	3.661389	0.001875	0.717086
-9.582497	-1.583387	3.671386	0.001752	0.717287
-9.484226	-1.556174	3.681382	0.001734	0.717376
-9.323252	-1.585852	3.691379	0.001703	0.717375
-9.015546	-1.600364	3.701376	0.001646	0.717455
-8.437530	-1.577939	3.711373	0.001538	0.717704
-8.287786	-1.604589	3.721370	0.001510	0.717705
-8.458464	-1.575431	3.731366	0.001541	0.717703
-7.890386	-1.564716	3.741363	0.001435	0.717925
-7.397222	-1.607084	3.751360	0.001343	0.718015
-7.387920	-1.607017	3.761357	0.001341	0.718019
-7.406325	-1.593431	3.771354	0.001344	0.718040
-6.723183	-1.557563	3.781350	0.001216	0.718352
-6.536756	-1.592129	3.791347	0.001181	0.718350
-6.370721	-1.620571	3.801344	0.001150	0.718353
-6.302949	-1.563035	3.811341	0.001137	0.718491
-5.452391	-1.637459	3.821338	0.000978	0.718644
-5.558680	-1.619852	3.831334	0.000998	0.718642
-5.435451	-1.642094	3.841331	0.000974	0.718642
-5.042099	-1.596692	3.851328	0.000901	0.718870
-4.872532	-1.580248	3.861325	0.000869	0.718963
-4.511863	-1.644579	3.871322	0.000801	0.718964
-4.684578	-1.599376	3.881318	0.000833	0.718993
-3.803230	-1.616612	3.891315	0.000669	0.719269
-3.732013	-1.628519	3.901312	0.000655	0.719271
-3.837350	-1.609934	3.911309	0.000674	0.719271
-3.405733	-1.603427	3.921306	0.000594	0.719437
-2.913284	-1.609358	3.931302	0.000502	0.719598
-2.832551	-1.623911	3.941299	0.000486	0.719599
-2.859300	-1.619520	3.951296	0.000491	0.719599
-2.403995	-1.573681	3.961293	0.000406	0.719849
-2.307920	-1.565382	3.971290	0.000387	0.719900
-2.122308	-1.600873	3.981286	0.000353	0.719896
-2.061893	-1.517389	3.991283	0.000341	0.720082
-1.885544	-1.478654	4.001280	0.000308	0.720221
-1.465387	-1.552462	4.011277	0.000229	0.720224
-1.407554	-1.465376	4.021274	0.000218	0.720416
-0.979533	-1.480160	4.031270	0.000138	0.720538
-1.428364	-1.400486	4.041267	0.000221	0.720538
-0.969577	-1.334955	4.051264	0.000135	0.720828
-1.220319	-1.265375	4.061261	0.000182	0.720878
-1.148841	-1.207130	4.071258	0.000168	0.721018
-0.918595	-1.195620	4.081254	0.000125	0.721122
-0.893291	-1.120702	4.091251	0.000120	0.721279
-0.792829	-1.058236	4.101248	0.000100	0.721438
-0.640998	-0.992175	4.111245	0.000072	0.721621
-0.497613	-0.954135	4.121242	0.000045	0.721747
-0.463897	-0.829208	4.131238	0.000038	0.722005
-0.536179	-0.762202	4.141235	0.000051	0.722112
-0.675671	-0.606168	4.151232	0.000077	0.722370
-0.580617	-0.514585	4.161229	0.000058	0.722584
-0.457785	-0.441019	4.171226	0.000035	0.722772
-0.415731	-0.329938	4.181222	0.000027	0.723005
-0.125018	-0.230213	4.191219	-0.000028	0.723303
-0.211249	-0.116496	4.201216	-0.000012	0.723496
-0.231792	0.006647	4.211213	-0.000009	0.723731
-0.153397	0.122108	4.221210	-0.000024	0.723985
0.000000	0.280518	4.231206	-0.000053	0.724350

0.210940	0.870415	4.236211	-0.000092	0.725578
0.229667	2.131030	4.241216	-0.000097	0.728044
0.564435	3.939472	4.246221	-0.000161	0.731674
0.939829	6.294798	4.251226	-0.000232	0.736355
1.099849	9.193243	4.256230	-0.000264	0.741971
1.465371	12.548261	4.261235	-0.000334	0.748479
2.191491	16.282096	4.266240	-0.000472	0.755763
2.644044	20.479091	4.271245	-0.000559	0.763748
3.228266	25.062870	4.276250	-0.000671	0.772403
3.721085	30.013437	4.281254	-0.000767	0.781598
4.470880	35.287135	4.286259	-0.000910	0.791347
4.888013	40.924228	4.291264	-0.000991	0.801516
5.487170	46.841462	4.296269	-0.001107	0.812103
6.051188	53.046355	4.301274	-0.001216	0.823038
6.617007	59.527308	4.306278	-0.001326	0.834300
7.060471	66.243706	4.311283	-0.001413	0.845770
7.559101	73.176583	4.316288	-0.001511	0.857460
8.082778	80.308256	4.321293	-0.001613	0.869324
8.875609	87.587951	4.326298	-0.001765	0.881343
9.558206	95.055427	4.331302	-0.001898	0.893466
10.223088	102.690756	4.336307	-0.002027	0.905685
10.502570	110.538330	4.341312	-0.002084	0.917965
11.062806	118.435769	4.346317	-0.002193	0.930233
12.624719	126.277837	4.351322	-0.002490	0.942521
13.845344	134.305652	4.356326	-0.002722	0.954837
14.333508	142.544533	4.361331	-0.002819	0.967118
14.701270	150.890560	4.366336	-0.002893	0.979370
15.786498	159.194753	4.371341	-0.003100	0.991588
16.586749	167.598464	4.376346	-0.003255	1.003728
16.882158	176.125051	4.381350	-0.003316	1.015771
17.806359	184.584204	4.386355	-0.003494	1.027730
18.708777	193.087061	4.391360	-0.003667	1.039606
19.858137	201.576250	4.396365	-0.003887	1.051386
20.590478	210.178449	4.401370	-0.004029	1.063090
21.387878	218.797189	4.406374	-0.004184	1.074702
22.125680	227.422161	4.411379	-0.004327	1.086185
22.846779	236.064662	4.416384	-0.004467	1.097566
23.826214	244.666854	4.421389	-0.004655	1.108835
24.495367	253.328256	4.426394	-0.004785	1.119997
25.212632	261.971508	4.431398	-0.004925	1.131037
25.935954	270.621664	4.436403	-0.005065	1.141979
26.377272	279.332077	4.441408	-0.005153	1.152832
27.035351	287.961404	4.446413	-0.005282	1.163529
27.339728	296.645461	4.451418	-0.005344	1.174122
28.138930	305.207783	4.456422	-0.005499	1.184576
28.846741	313.816139	4.461427	-0.005636	1.194974
29.363616	322.407523	4.466432	-0.005738	1.205223
29.822439	331.022416	4.471437	-0.005829	1.215402
30.487242	339.575633	4.476442	-0.005959	1.225465
30.989024	348.163114	4.481446	-0.006058	1.235453
31.856541	356.646188	4.486451	-0.006225	1.245313
33.012127	365.088964	4.491456	-0.006446	1.255104
33.611920	373.617754	4.496461	-0.006564	1.264810
34.074296	382.170835	4.501466	-0.006656	1.274444
34.681305	390.653920	4.506470	-0.006774	1.283954
35.445239	399.132587	4.511475	-0.006922	1.293418
35.785146	407.651262	4.516480	-0.006991	1.302779
36.506904	416.181354	4.521485	-0.007131	1.312155
37.067121	424.661338	4.526490	-0.007241	1.321381
37.526623	433.083865	4.531494	-0.007333	1.330464
37.582288	441.575613	4.536499	-0.007349	1.339486
38.387090	449.913325	4.541504	-0.007504	1.348418
39.028268	458.294609	4.546509	-0.007629	1.357308
39.504384	466.677718	4.551514	-0.007723	1.366113
39.985444	475.070546	4.556518	-0.007819	1.374872
40.371704	483.453158	4.561523	-0.007896	1.383549
40.799900	491.841776	4.566528	-0.007982	1.392185
41.018270	500.224022	4.571533	-0.008028	1.400726
41.959365	508.491581	4.576538	-0.008209	1.409220
42.633784	516.807711	4.581542	-0.008340	1.417667
43.147732	525.137051	4.586547	-0.008441	1.426051
43.552349	533.492223	4.591552	-0.008522	1.434393
43.924893	541.808824	4.596557	-0.008597	1.442644
44.346535	550.141579	4.601562	-0.008681	1.450871
44.731859	558.457043	4.606566	-0.008759	1.459029
45.363582	566.729889	4.611571	-0.008882	1.467140
45.618070	575.115856	4.616576	-0.008935	1.475254
46.293125	583.343871	4.621581	-0.009066	1.483240
47.026299	591.585656	4.626586	-0.009208	1.491204
46.966020	599.938897	4.631590	-0.009202	1.499109
47.217097	608.229791	4.636595	-0.009255	1.506961
47.896962	616.461723	4.641600	-0.009387	1.514783
48.621007	624.668526	4.646605	-0.009527	1.522547
49.112824	632.930487	4.651610	-0.009624	1.530288
49.668502	641.176625	4.656614	-0.009733	1.537985
50.248596	649.405160	4.661619	-0.009847	1.545631
50.753136	657.675469	4.666624	-0.009946	1.553266
51.247012	665.886002	4.671629	-0.010044	1.560807
51.964747	674.091914	4.676634	-0.010183	1.568341
52.438813	682.331842	4.681638	-0.010277	1.575833
52.845968	690.576498	4.686643	-0.010358	1.583285
53.325220	698.811933	4.691648	-0.010453	1.590703
53.753557	707.041598	4.696653	-0.010538	1.598075
54.166256	715.259241	4.701658	-0.010621	1.605400
54.692177	723.477943	4.706662	-0.010724	1.612708
55.325490	731.668094	4.711667	-0.010848	1.619973
55.581969	739.911764	4.716672	-0.010901	1.627199
55.617448	748.238724	4.721677	-0.010913	1.634435
56.190891	756.395237	4.726682	-0.011025	1.641566
56.836301	764.531360	4.731686	-0.011151	1.648659
57.232872	772.736677	4.736691	-0.011230	1.655746
57.606611	780.929023	4.741696	-0.011305	1.662789
58.061267	789.112598	4.746701	-0.011396	1.669805
58.477861	797.321639	4.751706	-0.011479	1.676808
58.803892	805.495382	4.756710	-0.011545	1.683740
59.215720	813.684784	4.761715	-0.011627	1.690668
59.592099	821.879051	4.766720	-0.011703	1.697567
59.916806	830.056809	4.771725	-0.011769	1.704417
60.545321	838.227330	4.776730	-0.011891	1.711274
60.950512	846.412104	4.781734	-0.011972	1.718086
61.436792	854.555653	4.786739	-0.012068	1.724847
61.925366	862.721406	4.791744	-0.012165	1.731600
62.380888	870.890069	4.796749	-0.012255	1.738325
62.525926	879.083116	4.801754	-0.012288	1.745004
62.686056	887.277378	4.806758	-0.012323	1.751661
63.395397	895.385238	4.811763	-0.012460	1.758292
63.765228	903.522537	4.816768	-0.012535	1.764879
63.917263	911.728085	4.821773	-0.012569	1.771468
64.908092	919.806018	4.826778	-0.012758	1.778036
65.281695	927.951123	4.831782	-0.012834	1.784556
65.742510	936.145463	4.836787	-0.012925	1.791102
66.065614	944.343248	4.841792	-0.012991	1.797610
66.485800	952.465353	4.846797	-0.013074	1.804046
66.750544	960.634145	4.851802	-0.013129	1.810478
66.988866	968.790273	4.856806	-0.013179	1.816873
67.626786	976.886231	4.861811	-0.013303	1.823247
67.884386	985.056413	4.866816	-0.013357	1.829611
68.255476	993.197167	4.871821	-0.013431	1.835943
68.808919	1001.304467	4.876826	-0.013540	1.842249
69.269828	1009.425138	4.881830	-0.013631	1.848533
69.629803	1017.590387	4.886835	-0.013703	1.854818
69.945250	1025.730580	4.891840	-0.013768	1.861057
70.204071	1033.868352	4.896845	-0.013821	1.867267
70.618463	1042.053118	4.901850	-0.013904	1.873510
70.707767	1050.189118	4.906854	-0.013926	1.879657
71.200197	1058.280718	4.911859	-0.014023	1.885798
71.619112	1066.408250	4.916864	-0.014107	1.891936
72.279217	1074.488701	4.921869	-0.014235	1.898048
72.620458	1082.631982	4.926874	-0.014304	1.904149
72.787110	1090.787497	4.931878	-0.014341	1.910221
73.153016	1098.919979	4.936883	-0.014414	1.916279
73.610991	1107.016299	4.941888	-0.014505	1.922301
74.026047	1115.129384	4.946893	-0.014588	1.928312
74.474859	1123.265005	4.951898	-0.014677	1.934324
74.784207	1131.373724	4.956902	-0.014740	1.940283
75.129910	1139.499621	4.961907	-0.014810	1.946239
75.421233	1147.679564	4.966912	-0.014869	1.952211
75.720691	1155.780813	4.971917	-0.014931	1.958108
76.235841	1163.853686	4.976922	-0.015032	1.963991
76.538721	1171.955792	4.981926	-0.015094	1.969853
77.075933	1180.052346	4.986931	-0.015199	1.975720
77.592359	1188.136542	4.991936	-0.015301	1.981558
77.999019	1196.232660	4.996941	-0.015382	1.987375
78.333806	1204.395426	5.001946	-0.015450	1.993215
78.324334	1212.524633	5.006950	-0.015454	1.998978
78.881709	1220.580651	5.011955	-0.015563	2.004732
79.275814	1228.689574	5.016960	-0.015642	2.010490
79.216371	1236.859144	5.021965	-0.015636	2.016226
79.759172	1244.932447	5.026970	-0.015743	2.021941
80.130711	1253.029045	5.031974	-0.015817	2.027639
80.500662	1261.169607	5.036979	-0.015892	2.033351
80.773991	1269.281020	5.041984	-0.015948	2.039016
81.055743	1277.341825	5.046989	-0.016006	2.044632
81.594494	1285.441834	5.051994	-0.016112	2.050285
81.789293	1293.545879	5.056998	-0.016153	2.055891
82.279756	1301.615538	5.062003	-0.016250	2.061487
82.727206	1309.706067	5.067008	-0.016339	2.067079
82.733471	1317.869311	5.072013	-0.016346	2.072660
83.036033	1325.963262	5.077018	-0.016407	2.078209
83.437765	1334.018926	5.082022	-0.016488	2.083727
83.745630	1342.130199	5.087027	-0.016550	2.089259
83.923554	1350.259674	5.092032	-0.016589	2.094775
84.183965	1358.343405	5.097037	-0.016643	2.100254
84.648802	1366.414228	5.102042	-0.016735	2.105730
84.829972	1374.562814	5.107046	-0.016774	2.111216
85.016401	1382.700471	5.112051	-0.016814	2.116682
85.356037	1390.757873	5.117056	-0.016883	2.122094
85.680186	1398.810656	5.122061	-0.016949	2.127488
86.018185	1406.911089	5.127066	-0.017017	2.132901
86.230809	1414.993524	5.132070	-0.017062	2.138276
86.785443	1423.035377	5.137075	-0.017171	2.143644
87.094743	1431.126073	5.142080	-0.017234	2.149007
87.284812	1439.237877	5.147085	-0.017275	2.154359
87.764344	1447.294132	5.152090	-0.017369	2.159689
87.891536	1455.380297	5.157094	-0.017399	2.164992
88.434682	1463.442733	5.162099	-0.017505	2.170305
88.839143	1471.536426	5.167104	-0.017586	2.175612
88.897161	1479.647903	5.172109	-0.017602	2.180887
89.128746	1487.747226	5.177114	-0.017651	2.186156
89.382931	1495.845185	5.182118	-0.017704	2.191414
89.708708	1503.926980	5.187123	-0.017770	2.196655
89.973720	1511.985654	5.192128	-0.017824	2.201864
90.224568	1520.066101	5.197133	-0.017877	2.207073
90.654892	1528.139583	5.202138	-0.017962	2.212281
90.967360	1536.210089	5.207142	-0.018026	2.217464
91.126567	1544.297701	5.212147	-0.018061	2.222632
91.472190	1552.379352	5.217152	-0.018131	2.227801
91.852114	1560.464147	5.222157	-0.018207	2.232963
91.942791	1568.569123	5.227162	-0.018229	2.238101
92.416067	1576.597787	5.232166	-0.018323	2.243212
92.712462	1584.672260	5.237171	-0.018383	2.248324
93.042705	1592.765349	5.242176	-0.018450	2.253440
93.108105	1600.863565	5.247181	-0.018468	2.258524
93.453665	1608.936688	5.252186	-0.018538	2.263605
93.704558	1617.015552	5.257190	-0.018590	2.268670
94.025417	1625.164443	5.262195	-0.018655	2.273774
94.291864	1633.202360	5.267200	-0.018710	2.278792
94.728189	1641.206260	5.272205	-0.018797	2.283793
95.010958	1649.283289	5.277210	-0.018855	2.288814
95.171599	1657.371036	5.282214	-0.018890	2.293821
95.552519	1665.420163	5.287219	-0.018966	2.298812
95.948415	1673.479665	5.292224	-0.019046	2.303800
96.090613	1681.563675	5.297229	-0.019078	2.308770
96.462829	1689.666919	5.302234	-0.019152	2.313761
96.690313	1697.706642	5.307238	-0.019200	2.318690
96.796932	1705.783474	5.312243	-0.019225	2.323621
97.213885	1713.841155	5.317248	-0.019308	2.328555
97.449574	1721.920555	5.322253	-0.019358	2.333478
97.825913	1729.996780	5.327258	-0.019433	2.338399
98.141492	1738.033884	5.332262	-0.019497	2.343282
98.414884	1746.112093	5.337267	-0.019554	2.348175
98.708059	1754.230643	5.342272	-0.019614	2.353085
98.964223	1762.287305	5.347277	-0.019667	2.357943
99.332581	1770.332852	5.352282	-0.019741	2.362794
99.281388	1778.417237	5.357286	-0.019737	2.367625
99.518842	1786.493932	5.362291	-0.019787	2.372464
100.150292	1794.525694	5.367296	-0.019909	2.377298
100.546321	1802.552977	5.372301	-0.019989	2.382101
100.762879	1810.637903	5.377306	-0.020034	2.386914
100.978655	1818.714065	5.382310	-0.020080	2.391712
101.349547	1826.776622	5.387315	-0.020155	2.396504
101.612808	1834.837862	5.392320	-0.020209	2.401278
101.763534	1842.893668	5.397325	-0.020242	2.406030
102.177283	1850.970178	5.402330	-0.020325	2.410805
102.448554	1859.038981	5.407334	-0.020381	2.415555
102.698972	1867.092427	5.412339	-0.020433	2.420285
102.886332	1875.169883	5.417344	-0.020473	2.425015
102.977682	1883.258506	5.422349	-0.020496	2.429735
103.239774	1891.414281	5.427354	-0.020550	2.434498
103.388219	1899.421614	5.432358	-0.020583	2.439157
103.596986	1907.453416	5.437363	-0.020627	2.443825
103.819222	1915.514086	5.442368	-0.020674	2.448502
104.047726	1923.569192	5.447373	-0.020722	2.453168
104.360232	1931.626884	5.452378	-0.020786	2.457832
104.625709	1939.661398	5.457382	-0.020841	2.462471
105.064926	1947.692085	5.462387	-0.020928	2.467112
105.386172	1955.773490	5.467392	-0.020993	2.471764
105.758691	1963.805433	5.472397	-0.021068	2.476383
105.971311	1971.881631	5.477402	-0.021113	2.481006
106.169363	1979.920605	5.482406	-0.021155	2.485599
106.443317	1987.984533	5.487411	-0.021212	2.490203
106.803347	1996.051598	5.492416	-0.021284	2.494806
106.809658	2004.126830	5.497421	-0.021291	2.499380
107.163078	2012.181185	5.502426	-0.021362	2.503958
107.434041	2020.242589	5.507430	-0.021418	2.508527
107.677716	2028.341799	5.512435	-0.021469	2.513106
108.085281	2036.375966	5.517440	-0.021550	2.517652
108.248898	2044.410555	5.522445	-0.021586	2.522172
108.597666	2052.446830	5.527450	-0.021656	2.526699
108.915933	2060.510866	5.532454	-0.021721	2.531231
109.170622	2068.581164	5.537459	-0.021774	2.535753
109.459823	2076.637521	5.542464	-0.021833	2.540262
109.720804	2084.661406	5.547469	-0.021887	2.544743
110.168463	2092.729907	5.552474	-0.021976	2.549254
110.379988	2100.815612	5.557478	-0.022021	2.553750
110.351741	2108.895256	5.562483	-0.022021	2.558218
110.535410	2116.938154	5.567488	-0.022060	2.562672
110.753793	2124.962158	5.572493	-0.022106	2.567111
111.134080	2133.038820	5.577498	-0.022183	2.571582
111.186669	2141.099388	5.582502	-0.022198	2.576014
111.460125	2149.133567	5.587507	-0.022254	2.580439
111.726942	2157.174271	5.592512	-0.022309	2.584860
111.893566	2165.232895	5.597517	-0.022346	2.589275
112.057856	2173.498113	5.602522	-0.022382	2.593796
112.279376	2181.482704	5.607526	-0.022428	2.598160
112.489252	2189.470822	5.612531	-0.022473	2.602518
112.808914	2197.476917	5.617536	-0.022538	2.606885
112.890974	2205.515816	5.622541	-0.022559	2.611247
113.328199	2213.556160	5.627546	-0.022645	2.615626
113.422675	2221.603287	5.632550	-0.022668	2.619979
113.768842	2229.604015	5.637555	-0.022738	2.624316
114.161052	2237.646459	5.642560	-0.022817	2.628671
114.413706	2245.710405	5.647565	-0.022869	2.633022
114.873553	2253.747176	5.652570	-0.022960	2.637364
115.005335	2261.794082	5.657574	-0.022990	2.641683
115.348640	2269.826802	5.662579	-0.023059	2.646001
115.745652	2277.889388	5.667584	-0.023139	2.650331
116.014719	2285.930947	5.672589	-0.023194	2.654635
116.593839	2293.970137	5.677594	-0.023308	2.658950
116.796275	2302.032833	5.682598	-0.023351	2.663247
117.029836	2310.087802	5.687603	-0.023400	2.667534
117.445278	2318.157941	5.692608	-0.023482	2.671835
117.740526	2326.215746	5.697613	-0.023543	2.676114
117.944925	2334.271601	5.702618	-0.023586	2.680379
118.229631	2342.264882	5.707622	-0.023645	2.684609
118.519403	2350.315465	5.712627	-0.023704	2.688864
118.632890	2358.409767	5.717632	-0.023731	2.693123
118.875214	2366.431140	5.722637	-0.023781	2.697346
119.090107	2374.497768	5.727642	-0.023827	2.701583
119.264709	2382.518689	5.732646	-0.023865	2.705788
119.601753	2390.562646	5.737651	-0.023933	2.710008
119.984031	2398.631915	5.742656	-0.024009	2.714238
120.110894	2406.665874	5.747661	-0.024038	2.718427
120.289116	2414.719406	5.752666	-0.024077	2.722623
120.587956	2422.746413	5.757670	-0.024138	2.726805
120.817876	2430.808598	5.762675	-0.024186	2.730996
121.032050	2438.878531	5.767680	-0.024232	2.735183
121.389792	2446.869524	5.772685	-0.024304	2.739331
121.803261	2454.934722	5.777690	-0.024386	2.743515
122.091656	2462.959281	5.782694	-0.024445	2.747664
122.273049	2471.098718	5.787699	-0.024484	2.751859
122.693716	2479.184164	5.792704	-0.024568	2.756034
123.035826	2487.154182	5.797709	-0.024637	2.760139
123.295026	2495.163091	5.802714	-0.024691	2.764253
123.441357	2503.218712	5.807718	-0.024724	2.768378
123.754175	2511.256554	5.812723	-0.024787	2.772498
123.957685	2519.319301	5.817728	-0.024830	2.776617
124.056715	2527.363943	5.822733	-0.024854	2.780715
124.651794	2535.338181	5.827738	-0.024971	2.784800
125.007994	2543.384259	5.832742	-0.025042	2.788902
125.084228	2551.455739	5.837747	-0.025062	2.792994
125.327154	2559.518570	5.842752	-0.025113	2.797086
125.546856	2567.539728	5.847757	-0.025159	2.801148
125.834003	2575.576653	5.852762	-0.025218	2.805217
126.176842	2583.622723	5.857766	-0.025287	2.809288
126.364094	2591.686128	5.862771	-0.025327	2.813353
126.571374	2599.745938	5.867776	-0.025371	2.817411
126.626435	2607.785078	5.872781	-0.025387	2.821444
127.035719	2615.810830	5.877786	-0.025469	2.825485
127.202624	2623.867868	5.882790	-0.025505	2.829521
127.403796	2631.925095	5.887795	-0.025548	2.833554
127.879410	2639.936976	5.892800	-0.025642	2.837574
127.944548	2647.993957	5.897805	-0.025659	2.841588
128.124342	2656.028621	5.902810	-0.025698	2.845591
128.369258	2664.050334	5.907814	-0.025749	2.849586
128.551746	2672.116351	5.912819	-0.025789	2.853594
128.754718	2680.168147	5.917824	-0.025832	2.857590
128.819359	2688.183703	5.922829	-0.025849	2.861555
129.334702	2696.203405	5.927834	-0.025951	2.865542
129.479216	2704.261622	5.932838	-0.025983	2.869521
129.483064	2712.348149	5.937843	-0.025989	2.873501
129.854044	2720.374305	5.942848	-0.026064	2.877466
130.111610	2728.374756	5.947853	-0.026117	2.881406
130.143043	2736.439570	5.952858	-0.026128	2.885361
130.358224	2744.461188	5.957862	-0.026174	2.889299
130.872436	2752.474710	5.962867	-0.026275	2.893243
131.141777	2760.550299	5.967872	-0.026331	2.897199
131.443460	2768.577096	5.972877	-0.026392	2.901128
131.860215	2776.593882	5.977882	-0.026475	2.905053
132.154843	2784.649357	5.982886	-0.026535	2.908984
132.448202	2792.756582	5.987891	-0.026596	2.912936
132.522737	2800.834593	5.992896	-0.026615	2.916856
132.652316	2808.814874	5.997901	-0.026644	2.920726
132.903638	2816.802818	6.002906	-0.026697	2.924601
133.128781	2824.841243	6.007910	-0.026744	2.928494
133.423094	2832.885535	6.012915	-0.026804	2.932389
133.594516	2840.950834	6.017920	-0.026841	2.936282
133.752346	2848.962151	6.022925	-0.026876	2.940143
133.834930	2857.004621	6.027930	-0.026897	2.944009
134.212075	2865.032305	6.032934	-0.026973	2.947880
134.392414	2873.079647	6.037939	-0.027012	2.951744
134.684890	2881.166018	6.042944	-0.027072	2.955627
134.807695	2889.146771	6.047949	-0.027100	2.959446
135.269983	2897.159651	6.052954	-0.027191	2.963293
135.366635	2905.221157	6.057958	-0.027215	2.967139
135.716660	2913.261422	6.062963	-0.027285	2.970984
136.100082	2921.306749	6.067968	-0.027362	2.974827
136.225404	2929.313253	6.072973	-0.027391	2.978633
136.497654	2937.362516	6.077978	-0.027447	2.982463
136.825313	2945.400542	6.082982	-0.027513	2.986285
136.893452	2953.427061	6.087987	-0.027531	2.990083
136.935882	2961.557191	6.092992	-0.027545	2.993925
137.139652	2969.538297	6.097997	-0.027588	2.997699
137.551864	2977.539390	6.103002	-0.027670	3.001488
137.797414	2985.559759	6.108006	-0.027721	3.005273
138.037450	2993.583641	6.113011	-0.027772	3.009055
138.514313	3001.654121	6.118016	-0.027866	3.012865
138.532753	3009.695822	6.123021	-0.027875	3.016635
138.828035	3017.739979	6.128026	-0.027935	3.020414
139.275203	3025.739075	6.133030	-0.028024	3.024175
139.424284	3033.780125	6.138035	-0.028057	3.027937
139.663444	3041.852030	6.143040	-0.028107	3.031712
140.056759	3049.870488	6.148045	-0.028185	3.035465
140.275424	3057.884953	6.153050	-0.028232	3.039204
140.221871	3065.945652	6.158054	-0.028227	3.042946
140.456847	3073.962880	6.163059	-0.028276	3.046677
141.022527	3082.005851	6.168064	-0.028387	3.050431
141.053089	3090.072257	6.173069	-0.028398	3.054166
141.052298	3098.122045	6.178074	-0.028403	3.057887
141.476220	3106.127276	6.183078	-0.028488	3.061603
141.700338	3114.148001	6.188083	-0.028535	3.065312
141.926662	3122.204792	6.193088	-0.028582	3.069034
142.054783	3130.313414	6.198093	-0.028612	3.072770
142.480128	3138.338505	6.203098	-0.028696	3.076477
142.596076	3146.328678	6.208102	-0.028723	3.080149
142.747619	3154.332342	6.213107	-0.028757	3.083825
143.124890	3162.350099	6.218112	-0.028832	3.087513
143.331922	3170.379801	6.223117	-0.028876	3.091194
143.409240	3178.433628	6.228122	-0.028896	3.094876
143.922094	3186.430688	6.233126	-0.028997	3.098547
144.256687	3194.448539	6.238131	-0.029065	3.102215
144.409426	3202.522424	6.243136	-0.029099	3.105897
144.533895	3210.529075	6.248141	-0.029127	3.109541
145.034748	3218.586759	6.253146	-0.029226	3.113222
145.159210	3226.651775	6.258150	-0.029255	3.116885
145.153503	3234.676524	6.263155	-0.029259	3.120519
145.309942	3242.684879	6.268160	-0.029293	3.124149
145.573098	3250.682388	6.273165	-0.029348	3.127775
145.946500	3258.753865	6.278170	-0.029423	3.131435
146.270109	3266.792771	6.283174	-0.029488	3.135073
146.393061	3274.843595	6.288179	-0.029517	3.138704
146.510759	3282.876543	6.293184	-0.029544	3.142322
146.646038	3290.889974	6.298189	-0.029575	3.145928
147.309566	3298.881175	6.303194	-0.029704	3.149542
147.376589	3306.983360	6.308198	-0.029722	3.153177
147.711505	3314.991374	6.313203	-0.029789	3.156776
148.012099	3323.011343	6.318208	-0.029851	3.160376
148.043796	3331.015659	6.323213	-0.029862	3.163952
148.128232	3339.082761	6.328218	-0.029883	3.167555
148.397773	3347.120173	6.333222	-0.029939	3.171149
148.762002	3355.117707	6.338227	-0.030012	3.174724
148.981319	3363.174230	6.343232	-0.030058	3.178316
149.082199	3371.206349	6.348237	-0.030082	3.181887
149.291697	3379.231502	6.353242	-0.030127	3.185456
149.339180	3387.287616	6.358246	-0.030141	3.189028
149.584100	3395.312059	6.363251	-0.030192	3.192591
149.959019	3403.369235	6.368256	-0.030267	3.196169
150.114966	3411.349657	6.373261	-0.030302	3.199700
150.367330	3419.358151	6.378266	-0.030354	3.203243
150.528485	3427.426110	6.383270	-0.030390	3.206805
150.699316	3435.435501	6.388275	-0.030427	3.210338
150.989491	3443.505779	6.393280	-0.030486	3.213898
151.164640	3451.516324	6.398285	-0.030524	3.217423
151.690999	3459.551173	6.403290	-0.030628	3.220970
151.817103	3467.558536	6.408294	-0.030656	3.224484
152.191151	3475.587900	6.413299	-0.030732	3.228014
152.316953	3483.681571	6.418304	-0.030760	3.231558
152.521104	3491.726119	6.423309	-0.030804	3.235080
152.738308	3499.708878	6.428314	-0.030850	3.238572
152.826299	3507.729556	6.433318	-0.030871	3.242071
153.082928	3515.724680	6.438323	-0.030925	3.245562
153.122970	3523.780879	6.443328	-0.030937	3.249067
153.185573	3531.832220	6.448333	-0.030955	3.252567
153.597077	3539.867371	6.453338	-0.031037	3.256070
153.889487	3547.841608	6.458342	-0.031096	3.259538
153.916530	3555.880539	6.463347	-0.031107	3.263020
154.204446	3563.937449	6.468352	-0.031166	3.266517
154.425750	3571.946320	6.473357	-0.031213	3.269986
154.561893	3580.008472	6.478362	-0.031243	3.273471
154.920263	3588.044615	6.483366	-0.031315	3.276950
155.108682	3596.017851	6.488371	-0.031356	3.280391
155.422016	3604.028192	6.493376	-0.031420	3.283850
155.563636	3612.101155	6.498381	-0.031451	3.287325
155.886244	3620.119146	6.503386	-0.031517	3.290780
155.946120	3628.186087	6.508390	-0.031533	3.294242
156.048778	3636.208135	6.513395	-0.031558	3.297682
156.553788	3644.245684	6.518400	-0.031657	3.301142
156.917083	3652.211043	6.523405	-0.031730	3.304561
156.925603	3660.283727	6.528410	-0.031737	3.308009
157.117237	3668.337586	6.533414	-0.031779	3.311452
157.499692	3676.371278	6.538419	-0.031855	3.314890
157.763554	3684.384377	6.543424	-0.031910	3.318312
157.720640	3692.391837	6.548429	-0.031907	3.321716
158.038344	3700.411018	6.553434	-0.031972	3.325135
158.345397	3708.434396	6.558438	-0.032034	3.328551
158.443514	3716.488919	6.563443	-0.032058	3.331970
158.760045	3724.536342	6.568448	-0.032122	3.335390
158.917438	3732.511583	6.573453	-0.032157	3.338770
159.224074	3740.552931	6.578458	-0.032219	3.342180
159.317575	3748.582706	6.583462	-0.032242	3.345574
159.347573	3756.615828	6.588467	-0.032253	3.348964
159.718828	3764.683172	6.593472	-0.032328	3.352377
159.695245	3772.736622	6.598477	-0.032329	3.355766
160.012755	3780.710143	6.603482	-0.032393	3.359131
160.460532	3788.703668	6.608486	-0.032482	3.362505
160.576648	3796.739098	6.613491	-0.032509	3.365881
160.812771	3804.761959	6.618496	-0.032559	3.369253
161.062682	3812.820141	6.623501	-0.032611	3.372637
161.274590	3820.882314	6.628506	-0.032655	3.376018
161.492802	3828.869191	6.633510	-0.032701	3.379364
161.644557	3836.883194	6.638515	-0.032735	3.382716
161.985239	3844.939412	6.643520	-0.032804	3.386089
162.157979	3852.961041	6.648525	-0.032841	3.389438
162.649031	3861.030665	6.653530	-0.032938	3.392815
162.913252	3869.109601	6.658534	-0.032993	3.396184
162.879654	3877.056259	6.663539	-0.032992	3.399484
163.237127	3885.049420	6.668544	-0.033064	3.402815
163.420978	3893.070345	6.673549	-0.033104	3.406147
163.578833	3901.093087	6.678554	-0.033138	3.409476
163.769997	3909.154196	6.683558	-0.033179	3.412819
163.930329	3917.180530	6.688563	-0.033215	3.416143
164.230526	3925.175225	6.693568	-0.033276	3.419455
164.388453	3933.188794	6.698573	-0.033311	3.422767
164.565586	3941.250300	6.703578	-0.033349	3.426097
164.891955	3949.241508	6.708582	-0.033415	3.429399
164.839696	3957.321681	6.713587	-0.033411	3.432722
165.080183	3965.384996	6.718592	-0.033461	3.436044
165.290947	3973.347604	6.723597	-0.033506	3.439321
165.688492	3981.351458	6.728602	-0.033585	3.442618
165.598014	3989.426374	6.733606	-0.033574	3.445924
165.727611	3997.416451	6.738611	-0.033603	3.449200
165.971487	4005.507288	6.743616	-0.033654	3.452518
166.161332	4013.540827	6.748621	-0.033695	3.455807
166.439842	4021.519147	6.753626	-0.033752	3.459074
166.972576	4029.543744	6.758630	-0.033857	3.462364
167.290963	4037.525142	6.763635	-0.033922	3.465627
167.769270	4045.575890	6.768640	-0.034016	3.468920
168.020666	4053.636437	6.773645	-0.034068	3.472207
168.380236	4061.681559	6.778650	-0.034141	3.475487
168.731393	4069.648946	6.783654	-0.034211	3.478733
168.449858	4077.703153	6.788659	-0.034164	3.481991
168.883546	4085.713856	6.793664	-0.034251	3.485250
169.163881	4093.735825	6.798669	-0.034308	3.488506
169.211455	4101.796022	6.803674	-0.034322	3.491768
169.477734	4109.821953	6.808678	-0.034377	3.495019
169.532246	4117.808548	6.813683	-0.034393	3.498245
169.810615	4125.853293	6.818688	-0.034450	3.501498
170.035874	4133.847758	6.823693	-0.034498	3.504726
170.125507	4141.893565	6.828698	-0.034520	3.507967
170.334517	4149.949298	6.833702	-0.034564	3.511214
170.378842	4157.942091	6.838707	-0.034578	3.514427
170.683149	4166.016409	6.843712	-0.034640	3.517677
170.833667	4174.017445	6.848717	-0.034673	3.520891
170.943831	4181.975942	6.853722	-0.034699	3.524083
171.159786	4190.064731	6.858726	-0.034745	3.527328
171.385479	4198.084581	6.863731	-0.034792	3.530542
171.662853	4206.136854	6.868736	-0.034849	3.533768
171.857673	4214.130101	6.873741	-0.034891	3.536965
172.057426	4222.173375	6.878746	-0.034933	3.540179
172.048475	4230.230355	6.883750	-0.034937	3.543389
172.154107	4238.218576	6.888755	-0.034962	3.546573
172.523353	4246.235132	6.893760	-0.035036	3.549773
172.847659	4254.340262	6.898765	-0.035102	3.553003
172.953912	4262.394427	6.903770	-0.035127	3.556204
173.291045	4270.337973	6.908774	-0.035196	3.559365
173.300174	4278.330375	6.913779	-0.035203	3.562533
173.511882	4286.363841	6.918784	-0.035247	3.565720
173.634864	4294.376398	6.923789	-0.035276	3.568894
173.914833	4302.417013	6.928794	-0.035333	3.572080
174.317937	4310.445636	6.933798	-0.035414	3.575263
174.217017	4318.461447	6.938803	-0.035400	3.578422
174.473800	4326.479621	6.943808	-0.035454	3.581591
174.670090	4334.472144	6.948813	-0.035496	3.584744
175.011559	4342.486673	6.953818	-0.035565	3.587908
175.350839	4350.557853	6.958822	-0.035633	3.591090
175.573520	4358.528672	6.963827	-0.035680	3.594228
175.840244	4366.599693	6.968832	-0.035735	3.597403
175.929716	4374.605457	6.973837	-0.035757	3.600545
175.892246	4382.599437	6.978842	-0.035755	3.603675
176.119789	4390.670824	6.983846	-0.035803	3.606841
176.495498	4398.644628	6.988851	-0.035879	3.609970
176.705185	4406.698059	6.993856	-0.035923	3.613122
176.679864	4414.768854	6.998861	-0.035924	3.616273
176.740999	4422.749295	7.003866	-0.035941	3.619387
177.331877	4430.778711	7.008870	-0.036056	3.622532
177.364096	4438.798433	7.013875	-0.036067	3.625656
177.443842	4446.839429	7.018880	-0.036088	3.628786
177.707225	4454.881025	7.023885	-0.036142	3.631919
178.059940	4462.900956	7.028890	-0.036213	3.635044
178.303452	4470.889649	7.033894	-0.036264	3.638150
178.307872	4478.977561	7.038899	-0.036270	3.641286
178.625910	4486.908900	7.043904	-0.036335	3.644367
178.738242	4494.981499	7.048909	-0.036361	3.647494
178.920752	4502.981151	7.053914	-0.036400	3.650592
179.006372	4511.050907	7.058918	-0.036422	3.653712
179.037851	4519.064954	7.063923	-0.036433	3.656807
179.284523	4527.086557	7.068928	-0.036484	3.659907
179.309288	4535.121219	7.073933	-0.036494	3.663004
179.627285	4543.135563	7.078938	-0.036559	3.666098
180.018439	4551.157577	7.083942	-0.036637	3.669195
179.951087	4559.197071	7.088947	-0.036630	3.672283
180.194671	4567.228966	7.093952	-0.036681	3.675375
180.319809	4575.217058	7.098957	-0.036710	3.678443
180.637055	4583.239804	7.103962	-0.036774	3.681527
180.624768	4591.269320	7.108966	-0.036777	3.684603
180.808435	4599.301535	7.113971	-0.036817	3.687682
181.167391	4607.301203	7.118976	-0.036889	3.690751
181.416146	4615.345198	7.123981	-0.036941	3.693831
181.512574	4623.365949	7.128986	-0.036964	3.696896
181.543014	4631.377262	7.133990	-0.036975	3.699953
181.802814	4639.353203	7.138995	-0.037029	3.703000
182.168103	4647.448696	7.144000	-0.037102	3.706092
182.352422	4655.440576	7.149005	-0.037142	3.709138
182.415388	4663.526648	7.154010	-0.037159	3.712214
182.848472	4671.601335	7.159014	-0.037245	3.715292
183.026542	4679.544638	7.164019	-0.037284	3.718312
183.384243	4687.566133	7.169024	-0.037356	3.721363
183.422846	4695.513409	7.174029	-0.037368	3.724376
183.565722	4703.542155	7.179034	-0.037400	3.727420
183.718958	4711.585956	7.184038	-0.037434	3.730467
183.778705	4719.600197	7.189043	-0.037451	3.733498
184.035248	4727.645763	7.194048	-0.037504	3.736543
184.273248	4735.641253	7.199053	-0.037554	3.739566
184.246027	4743.682336	7.204058	-0.037554	3.742598
184.343077	4751.719672	7.209062	-0.037578	3.745629
184.737586	4759.722613	7.214067	-0.037656	3.748651
184.835941	4767.787973	7.219072	-0.037680	3.751688
184.945549	4775.785269	7.224077	-0.037706	3.754697
185.371897	4783.771123	7.229082	-0.037791	3.757706
185.570654	4791.825865	7.234086	-0.037833	3.760733
185.425421	4799.830023	7.239091	-0.037812	3.763731
185.551294	4807.892265	7.244096	-0.037840	3.766755
185.848794	4815.898016	7.249101	-0.037901	3.769759
185.922055	4823.920591	7.254106	-0.037920	3.772762
186.024433	4832.000474	7.259110	-0.037945	3.775784
186.333420	4839.938921	7.264115	-0.038008	3.778756
186.580987	4848.015510	7.269120	-0.038059	3.781776
186.671268	4856.018492	7.274125	-0.038081	3.784762
187.052402	4864.010433	7.279130	-0.038158	3.787748
187.135354	4872.093758	7.284134	-0.038179	3.790759
187.323577	4880.104249	7.289139	-0.038219	3.793743
187.450892	4888.147434	7.294144	-0.038248	3.796736
187.781820	4896.089974	7.299149	-0.038315	3.799693
187.932564	4904.123522	7.304154	-0.038349	3.802677
187.953959	4912.166834	7.309158	-0.038358	3.805660
188.113791	4920.145157	7.314163	-0.038393	3.808620
188.361392	4928.200569	7.319168	-0.038445	3.811608
188.651920	4936.210956	7.324173	-0.038504	3.814577
188.650227	4944.237882	7.329178	-0.038509	3.817545
189.115468	4952.256795	7.334182	-0.038601	3.820516
189.038663	4960.238871	7.339187	-0.038592	3.823461
189.131638	4968.321507	7.344192	-0.038615	3.826444
189.595117	4976.282542	7.349197	-0.038707	3.829387
189.490516	4984.380644	7.354202	-0.038693	3.832367
189.736424	4992.381086	7.359206	-0.038744	3.835315
189.849900	5000.377446	7.364211	-0.038770	3.838258
190.105175	5008.411117	7.369216	-0.038823	3.841214
190.066211	5016.379131	7.374221	-0.038822	3.844138
190.278075	5024.435384	7.379226	-0.038866	3.847098
190.763120	5032.432429	7.384230	-0.038962	3.850038
190.744010	5040.498787	7.389235	-0.038964	3.852992
190.755576	5048.539765	7.394240	-0.038972	3.855935
190.914196	5056.557430	7.399245	-0.039006	3.858870
191.188987	5064.516763	7.404250	-0.039063	3.861784
191.430792	5072.559317	7.409254	-0.039113	3.864725
191.412434	5080.642860	7.414259	-0.039115	3.867674
191.603769	5088.647485	7.419264	-0.039156	3.870596
191.749717	5096.872484	7.424269	-0.039189	3.873595
191.860486	5104.841549	7.429274	-0.039215	3.876497
192.030538	5112.773951	7.434278	-0.039252	3.879386
192.400594	5120.716228	7.439283	-0.039326	3.882280
192.566307	5128.754634	7.444288	-0.039363	3.885202
192.606953	5136.773125	7.449293	-0.039376	3.888113
192.780103	5144.789760	7.454298	-0.039413	3.891023
192.966160	5152.842826	7.459302	-0.039453	3.893945
192.978724	5160.856820	7.464307	-0.039461	3.896847
193.257988	5168.848135	7.469312	-0.039519	3.899743
193.602332	5176.864578	7.474317	-0.039588	3.902648
193.493217	5184.864075	7.479322	-0.039573	3.905536
193.987300	5192.879692	7.484326	-0.039670	3.908439
194.124272	5200.914747	7.489331	-0.039701	3.911340
194.313690	5208.935804	7.494336	-0.039742	3.914234
194.280815	5216.997701	7.499341	-0.039741	3.917137
194.544850	5224.946271	7.504346	-0.039796	3.920003
194.673605	5232.982345	7.509350	-0.039825	3.922896
194.777350	5240.993526	7.514355	-0.039850	3.925777
194.973823	5249.023354	7.519360	-0.039892	3.928664
195.223527	5257.073039	7.524365	-0.039944	3.931557
195.255662	5265.068252	7.529370	-0.039955	3.934425
195.572008	5273.089994	7.534374	-0.040020	3.937305
195.696665	5281.076695	7.539379	-0.040048	3.940167
195.803680	5289.107671	7.544384	-0.040074	3.943042
196.138754	5297.104482	7.549389	-0.040141	3.945907
196.538718	5305.105815	7.554394	-0.040221	3.948773
196.693307	5313.204758	7.559398	-0.040255	3.951667
196.673770	5321.247289	7.564403	-0.040257	3.954536
197.035029	5329.243877	7.569408	-0.040330	3.957393
197.314587	5337.207395	7.574413	-0.040387	3.960234
197.248564	5345.215341	7.579418	-0.040380	3.963084
197.713954	5353.255336	7.584422	-0.040472	3.965952
197.869529	5361.248504	7.589427	-0.040507	3.968795
197.875853	5369.297665	7.594432	-0.040513	3.971654
198.073610	5377.346204	7.599437	-0.040556	3.974515
198.199602	5385.370559	7.604442	-0.040584	3.977363
198.509224	5393.397382	7.609446	-0.040648	3.980213
198.463896	5401.394685	7.614451	-0.040644	3.983044
198.551535	5409.433827	7.619456	-0.040666	3.985891
198.702906	5417.434297	7.624461	-0.040700	3.988723
198.790141	5425.472651	7.629466	-0.040721	3.991565
199.144008	5433.538112	7.634470	-0.040793	3.994420
199.239824	5441.523979	7.639475	-0.040816	3.997239
199.307404	5449.553131	7.644480	-0.040834	4.000072
199.354482	5457.552607	7.649485	-0.040848	4.002892
199.602237	5465.586804	7.654490	-0.040900	4.005725
199.806517	5473.594149	7.659494	-0.040943	4.008546
199.919122	5481.629991	7.664499	-0.040969	4.011374
200.148569	5489.662784	7.669504	-0.041018	4.014200
200.533148	5497.688218	7.674509	-0.041095	4.017024
200.505717	5505.680752	7.679514	-0.041095	4.019828
200.816346	5513.719179	7.684518	-0.041158	4.022652
201.100078	5521.695053	7.689523	-0.041216	4.025451
201.178738	5529.747107	7.694528	-0.041236	4.028272
201.119823	5537.809046	7.699533	-0.041231	4.031092
201.297374	5545.889595	7.704538	-0.041269	4.033920
201.578823	5553.889190	7.709542	-0.041327	4.036720
201.828335	5561.784033	7.714547	-0.041379	4.039480
202.004401	5569.836100	7.719552	-0.041417	4.042292
202.425105	5577.832400	7.724557	-0.041501	4.045087
202.538733	5585.849204	7.729562	-0.041527	4.047882
202.591555	5593.918116	7.734566	-0.041543	4.050692
202.591312	5601.915905	7.739571	-0.041548	4.053475
202.783068	5609.946209	7.744576	-0.041589	4.056270
202.858068	5617.898913	7.749581	-0.041608	4.059035
203.011353	5625.940180	7.754586	-0.041642	4.061829
203.255184	5633.950029	7.759590	-0.041693	4.064612
203.387662	5641.985349	7.764595	-0.041723	4.067401
203.620904	5650.004113	7.769600	-0.041772	4.070183
203.957251	5658.048636	7.774605	-0.041840	4.072973
204.009655	5666.072385	7.779610	-0.041855	4.075750
204.148436	5674.058428	7.784614	-0.041887	4.078514
204.307483	5682.069928	7.789619	-0.041922	4.081285
204.282152	5690.072580	7.794624	-0.041922	4.084048
204.583883	5698.112039	7.799629	-0.041984	4.086827
204.679976	5706.100911	7.804634	-0.042007	4.089583
204.920096	5714.205565	7.809638	-0.042057	4.092380
204.850445	5722.191029	7.814643	-0.042050	4.095129
205.076178	5730.199406	7.819648	-0.042097	4.097888
205.315994	5738.226359	7.824653	-0.042147	4.100652
205.381241	5746.211025	7.829658	-0.042165	4.103397
205.597330	5754.265318	7.834662	-0.042210	4.106166
205.765138	5762.288768	7.839667	-0.042247	4.108922
205.881248	5770.352417	7.844672	-0.042274	4.111690
206.013321	5778.383598	7.849677	-0.042304	4.114444
205.997969	5786.379248	7.854682	-0.042307	4.117183
206.367123	5794.362242	7.859686	-0.042381	4.119920
206.531135	5802.340052	7.864691	-0.042417	4.122651
206.425678	5810.353266	7.869696	-0.042402	4.125389
206.852635	5818.400684	7.874701	-0.042487	4.128144
206.977128	5826.397006	7.879706	-0.042516	4.130875
207.011264	5834.505401	7.884710	-0.042528	4.133642
206.832480	5842.510603	7.889715	-0.042500	4.136369
207.327324	5850.495914	7.894720	-0.042597	4.139096
207.441596	5858.523227	7.899725	-0.042624	4.141831
207.489464	5866.510530	7.904730	-0.042638	4.144549
207.704862	5874.575255	7.909734	-0.042684	4.147294
207.819299	5882.547869	7.914739	-0.042710	4.150004
207.927939	5890.619759	7.919744	-0.042736	4.152747
208.154214	5898.675466	7.924749	-0.042784	4.155483
208.326820	5906.623326	7.929754	-0.042821	4.158180
208.549276	5914.654883	7.934758	-0.042868	4.160905
208.732434	5922.641508	7.939763	-0.042908	4.163612
208.911368	5930.667698	7.944768	-0.042946	4.166331
209.080512	5938.683845	7.949773	-0.042983	4.169044
209.176820	5946.708662	7.954778	-0.043006	4.171758
209.456468	5954.754820	7.959782	-0.043064	4.174479
209.621907	5962.759259	7.964787	-0.043100	4.177183
209.803273	5970.748993	7.969792	-0.043139	4.179880
209.948956	5978.798869	7.974797	-0.043172	4.182596
210.032350	5986.755965	7.979802	-0.043193	4.185278
210.081960	5994.829678	7.984806	-0.043207	4.187996
210.141482	6002.833168	7.989811	-0.043224	4.190690
210.436850	6010.968957	7.994816	-0.043284	4.193429
210.595003	6019.003967	7.999821	-0.043319	4.196131
210.836709	6026.864894	8.004826	-0.043370	4.198773
210.902900	6034.931810	8.009830	-0.043387	4.201481
210.886693	6042.894802	8.014835	-0.043390	4.204152
211.089672	6050.907299	8.019840	-0.043433	4.206840
211.238645	6058.922948	8.024845	-0.043466	4.209526
211.425421	6066.961286	8.029850	-0.043506	4.212219
211.621890	6074.999889	8.034854	-0.043548	4.214910
211.682573	6083.008594	8.039859	-0.043565	4.217588
211.983760	6091.008645	8.044864	-0.043626	4.220264
212.097926	6099.021363	8.049869	-0.043653	4.222940
212.320274	6107.023841	8.054874	-0.043700	4.225613
212.513230	6115.078240	8.059878	-0.043741	4.228301
212.679079	6123.070234	8.064883	-0.043777	4.230966
212.763693	6131.120343	8.069888	-0.043799	4.233647
212.855917	6139.159427	8.074893	-0.043821	4.236324
212.954533	6147.146183	8.079898	-0.043845	4.238981
213.173196	6155.213495	8.084902	-0.043891	4.241665
213.077632	6163.132273	8.089907	-0.043879	4.244295
213.217189	6171.196066	8.094912	-0.043910	4.246973
213.396840	6179.151880	8.099917	-0.043949	4.249614
213.529686	6187.209153	8.104922	-0.043979	4.252287
213.676964	6195.274930	8.109926	-0.044012	4.254961
213.781126	6203.264036	8.114931	-0.044037	4.257607
213.785710	6211.282572	8.119936	-0.044043	4.260261
214.000253	6219.299513	8.124941	-0.044088	4.262915
214.254958	6227.301571	8.129946	-0.044141	4.265562
214.405262	6235.371048	8.134950	-0.044174	4.268229
214.612139	6243.355222	8.139955	-0.044218	4.270866
214.848333	6251.413706	8.144960	-0.044268	4.273527
214.813217	6259.502362	8.149965	-0.044267	4.276193
214.959951	6267.394226	8.154970	-0.044299	4.278795
215.319695	6275.505536	8.159974	-0.044372	4.281469
215.515179	6283.428851	8.164979	-0.044413	4.284078
215.530241	6291.492673	8.169984	-0.044422	4.286730
215.697764	6299.485476	8.174989	-0.044458	4.289358
215.842237	6307.514254	8.179994	-0.044491	4.291997
216.097655	6315.611902	8.184998	-0.044544	4.294657
216.062058	6323.576143	8.190003	-0.044542	4.297269
216.320731	6331.544761	8.195008	-0.044596	4.299884
216.598271	6339.609386	8.200013	-0.044653	4.302529
216.583976	6347.625015	8.205018	-0.044656	4.305153
216.886474	6355.632320	8.210022	-0.044717	4.307776
216.979701	6363.654318	8.215027	-0.044740	4.310401
217.002777	6371.703901	8.220032	-0.044750	4.313032
217.011188	6379.699482	8.225037	-0.044757	4.315644
217.170243	6387.663946	8.230042	-0.044792	4.318245
217.324704	6395.743468	8.235046	-0.044826	4.320882
217.293340	6403.673180	8.240051	-0.044826	4.323467
217.590689	6411.759396	8.245056	-0.044886	4.326105
217.911474	6419.721657	8.250061	-0.044951	4.328700
217.816603	6427.771819	8.255066	-0.044939	4.331319
217.978401	6435.813572	8.260070	-0.044975	4.333936
218.119381	6443.829965	8.265075	-0.045006	4.336543
218.311445	6451.772292	8.270080	-0.045047	4.339125
218.519126	6459.863384	8.275085	-0.045092	4.341753
218.658447	6467.754937	8.280090	-0.045123	4.344315
218.972708	6475.897008	8.285094	-0.045187	4.346957
218.990927	6483.867160	8.290099	-0.045196	4.349540
219.247592	6491.952917	8.295104	-0.045249	4.352161
219.408679	6500.062952	8.300109	-0.045284	4.354787
219.531939	6507.992395	8.305114	-0.045313	4.357353
219.727849	6515.981158	8.310118	-0.045354	4.359937
219.726319	6523.935115	8.315123	-0.045360	4.362507
219.930322	6531.946847	8.320128	-0.045403	4.365096
220.053525	6540.004648	8.325133	-0.045431	4.367697
220.023771	6547.998563	8.330138	-0.045431	4.370275
220.527772	6556.054985	8.335142	-0.045530	4.372875
220.456787	6564.062151	8.340147	-0.045523	4.375454
220.597266	6572.072071	8.345152	-0.045554	4.378034
220.921232	6580.091205	8.350157	-0.045620	4.380616
220.856896	6588.025086	8.355162	-0.045613	4.383167
220.959164	6596.128708	8.360166	-0.045638	4.385772
221.350732	6604.144595	8.365171	-0.045716	4.388349
221.385916	6612.148218	8.370176	-0.045728	4.390918
221.490000	6620.189435	8.375181	-0.045753	4.393499
221.540694	6628.200299	8.380186	-0.045768	4.396067
221.884324	6636.214844	8.385190	-0.045837	4.398637
221.813685	6644.220637	8.390195	-0.045829	4.401201
222.012826	6652.199319	8.395200	-0.045872	4.403756
222.230522	6660.236117	8.400205	-0.045918	4.406328
222.222548	6668.242254	8.405210	-0.045922	4.408887
222.417339	6676.303591	8.410214	-0.045963	4.411464
222.655373	6684.345577	8.415219	-0.046013	4.414033
222.643826	6692.361962	8.420224	-0.046016	4.416591
222.880613	6700.341017	8.425229	-0.046066	4.419137
222.833070	6708.357476	8.430234	-0.046062	4.421692
223.253421	6716.323559	8.435238	-0.046146	4.424232
223.101192	6724.398935	8.440243	-0.046123	4.426802
223.359779	6732.444532	8.445248	-0.046176	4.429363
223.786997	6740.469899	8.450253	-0.046261	4.431917
223.911320	6748.484696	8.455258	-0.046290	4.434465
223.961273	6756.542554	8.460262	-0.046305	4.437025
224.094335	6764.485907	8.465267	-0.046335	4.439547
224.466381	6772.495566	8.470272	-0.046410	4.442090
224.354328	6780.499684	8.475277	-0.046394	4.444628
224.616814	6788.509330	8.480282	-0.046448	4.447167
224.909086	6796.571595	8.485286	-0.046508	4.449722
224.883884	6804.574592	8.490291	-0.046509	4.452255
224.847805	6812.594127	8.495296	-0.046508	4.454792
225.030714	6820.666880	8.500301	-0.046547	4.457345
225.209584	6828.576388	8.505306	-0.046586	4.459845
225.552516	6836.625894	8.510310	-0.046655	4.462389
225.501970	6844.609577	8.515315	-0.046651	4.464908
225.793305	6852.684873	8.520320	-0.046711	4.467457
225.923666	6860.711269	8.525325	-0.046740	4.469988
225.805994	6868.711352	8.530330	-0.046724	4.472508
226.107223	6876.737085	8.535334	-0.046785	4.475037
226.090883	6884.723289	8.540339	-0.046788	4.477550
226.308920	6892.722416	8.545344	-0.046834	4.480067
226.725493	6900.772741	8.550349	-0.046917	4.482600
226.703788	6908.749776	8.555354	-0.046918	4.485106
226.928212	6916.795435	8.560359	-0.046965	4.487633
226.966145	6924.806762	8.565363	-0.046978	4.490148
227.329412	6932.847345	8.570368	-0.047051	4.492671
227.381805	6940.896531	8.575373	-0.047066	4.495194
227.190903	6948.860820	8.580378	-0.047036	4.497689
227.523130	6956.877584	8.585383	-0.047103	4.500201
227.675696	6964.869624	8.590387	-0.047137	4.502702
227.649528	6972.901670	8.595392	-0.047137	4.505214
228.018745	6980.933850	8.600397	-0.047211	4.507726
228.171187	6988.901492	8.605402	-0.047245	4.510216
228.312597	6997.064708	8.610407	-0.047277	4.512766
228.323104	7005.067530	8.615411	-0.047284	4.515263
228.518249	7012.975258	8.620416	-0.047326	4.517730
228.792574	7021.008010	8.625421	-0.047382	4.520235
228.759033	7028.983433	8.630426	-0.047382	4.522720
229.094674	7036.982677	8.635431	-0.047449	4.525212
229.162332	7045.034479	8.640435	-0.047467	4.527718
229.192941	7052.997656	8.645440	-0.047479	4.530195
229.456278	7061.078210	8.650445	-0.047533	4.532707
229.689829	7069.091181	8.655450	-0.047582	4.535197
229.903901	7077.122854	8.660455	-0.047627	4.537692
229.978728	7085.087418	8.665459	-0.047646	4.540164
230.164340	7093.144319	8.670464	-0.047686	4.542663
230.175305	7101.121085	8.675469	-0.047694	4.545136
230.211983	7109.139361	8.680474	-0.047706	4.547621
230.556953	7117.145328	8.685479	-0.047776	4.550100
230.731271	7125.225264	8.690483	-0.047814	4.552601
230.794871	7133.238570	8.695488	-0.047831	4.555080
231.167056	7141.253853	8.700493	-0.047906	4.557559
231.292835	7149.212071	8.705498	-0.047934	4.560018
231.425151	7157.248433	8.710503	-0.047964	4.562500
231.584850	7165.253709	8.715507	-0.047999	4.564971
232.034975	7173.283551	8.720512	-0.048089	4.567449
232.184459	7181.280530	8.725517	-0.048122	4.569915
231.904466	7189.332001	8.730522	-0.048075	4.572395
232.231001	7197.403035	8.735527	-0.048141	4.574881
232.467198	7205.378428	8.740531	-0.048191	4.577336
232.800053	7213.320373	8.745536	-0.048258	4.579780
232.847503	7221.419791	8.750541	-0.048272	4.582270
232.809266	7229.352114	8.755546	-0.048271	4.584708
232.968979	7237.458004	8.760551	-0.048306	4.587198
233.125459	7245.492079	8.765555	-0.048340	4.589664
233.434270	7253.499728	8.770560	-0.048403	4.592121
233.738523	7261.544391	8.775565	-0.048465	4.594588
233.548484	7269.516784	8.780570	-0.048435	4.597032
233.820136	7277.512141	8.785575	-0.048491	4.599481
234.050488	7285.600660	8.790579	-0.048540	4.601957
234.072470	7293.521336	8.795584	-0.048549	4.604381
234.262590	7301.607427	8.800589	-0.048590	4.606854
234.486553	7309.485419	8.805594	-0.048637	4.609262
234.765372	7317.581253	8.810599	-0.048694	4.611735
234.873053	7325.642702	8.815603	-0.048720	4.614196
234.804380	7333.670623	8.820608	-0.048712	4.616646
235.197765	7341.646615	8.825613	-0.048791	4.619079
235.317210	7349.655521	8.830618	-0.048819	4.621520
235.336421	7357.649173	8.835623	-0.048828	4.623956
235.473554	7365.694332	8.840627	-0.048859	4.626406
235.649001	7373.676139	8.845632	-0.048897	4.628835
235.688100	7381.781128	8.850637	-0.048909	4.631300
235.869457	7389.773573	8.855642	-0.048948	4.633730
236.018069	7397.765098	8.860647	-0.048982	4.636158
236.144332	7405.749527	8.865651	-0.049010	4.638583
236.278742	7413.749524	8.870656	-0.049041	4.641012
236.570903	7421.798386	8.875661	-0.049101	4.643453
236.479747	7429.782700	8.880666	-0.049089	4.645874
236.696718	7437.794632	8.885671	-0.049135	4.648302
236.985798	7445.848164	8.890675	-0.049194	4.650742
237.039387	7453.900174	8.895680	-0.049210	4.653179
237.211918	7461.899025	8.900685	-0.049247	4.655599
237.227380	7469.856143	8.905690	-0.049255	4.658006
237.359470	7477.897361	8.910695	-0.049285	4.660436
237.542208	7485.876874	8.915699	-0.049325	4.662847
237.654214	7493.937877	8.920704	-0.049351	4.665281
238.056486	7501.972281	8.925709	-0.049431	4.667705
238.119621	7509.946386	8.930714	-0.049448	4.670110
238.207743	7518.064586	8.935719	-0.049470	4.672558
238.464773	7526.106018	8.940723	-0.049524	4.674980
238.425435	7534.031010	8.945728	-0.049522	4.677367
238.736862	7542.039662	8.950733	-0.049585	4.679777
238.847769	7550.070181	8.955738	-0.049611	4.682193
239.118505	7557.983240	8.960743	-0.049667	4.684572
239.122770	7566.032940	8.965747	-0.049673	4.686991
239.139106	7574.017228	8.970752	-0.049681	4.689390
239.419760	7582.097732	8.975757	-0.049739	4.691815
239.617136	7590.109159	8.980762	-0.049781	4.694219
239.831328	7598.159247	8.985767	-0.049827	4.696633
239.907133	7606.113669	8.990771	-0.049846	4.699017
240.103278	7614.125116	8.995776	-0.049888	4.701417
240.312790	7622.164820	9.000781	-0.049932	4.703824
240.191544	7630.145800	9.005786	-0.049915	4.706213
240.425047	7638.164774	9.010791	-0.049964	4.708611
240.515193	7646.228609	9.015795	-0.049986	4.711022
240.548616	7654.263776	9.020800	-0.049998	4.713423
240.782263	7662.301544	9.025805	-0.050047	4.715823
240.871234	7670.222011	9.030810	-0.050069	4.718188
240.993419	7678.218988	9.035815	-0.050097	4.720573
241.204467	7686.269004	9.040819	-0.050142	4.722974
241.407154	7694.274938	9.045824	-0.050185	4.725359
241.654664	7702.364026	9.050829	-0.050236	4.727769
241.708543	7710.318167	9.055834	-0.050252	4.730137
242.140979	7718.432045	9.060839	-0.050338	4.732551
242.063531	7726.392050	9.065843	-0.050329	4.734919
242.043996	7734.422759	9.070848	-0.050330	4.737306
242.384325	7742.407537	9.075853	-0.050399	4.739678
242.619326	7750.455306	9.080858	-0.050448	4.742068
242.724268	7758.431190	9.085863	-0.050473	4.744435
242.723489	7766.484708	9.090867	-0.050478	4.746825
243.146020	7774.419457	9.095872	-0.050562	4.749177
243.359014	7782.557227	9.100877	-0.050608	4.751588
243.467236	7790.538883	9.105882	-0.050633	4.753952
243.738253	7798.588639	9.110887	-0.050689	4.756335
243.995713	7806.536874	9.115891	-0.050742	4.758686
243.963622	7814.517403	9.120896	-0.050742	4.761047
244.188188	7822.574672	9.125901	-0.050789	4.763429
244.386918	7830.558614	9.130906	-0.050831	4.765787
244.417947	7838.581523	9.135911	-0.050842	4.768157
244.527463	7846.597794	9.140915	-0.050868	4.770523
244.849765	7854.620811	9.145920	-0.050934	4.772889
244.934436	7862.639568	9.150925	-0.050955	4.775254
244.975025	7870.625742	9.155930	-0.050968	4.777608
245.391803	7878.669654	9.160935	-0.051051	4.779976
245.446788	7886.674649	9.165939	-0.051066	4.782333
245.433729	7894.696481	9.170944	-0.051069	4.784695
245.737438	7902.724568	9.175949	-0.051131	4.787055
245.774323	7910.721113	9.180954	-0.051144	4.789406
246.107037	7918.718408	9.185959	-0.051211	4.791755
246.228084	7926.770907	9.190963	-0.051239	4.794120
246.368600	7934.800069	9.195968	-0.051270	4.796477
246.607571	7942.746388	9.200973	-0.051320	4.798808
246.538933	7950.786778	9.205978	-0.051313	4.801167
246.872059	7958.786121	9.210983	-0.051380	4.803510
247.073977	7966.832233	9.215987	-0.051423	4.805867
247.113448	7974.778540	9.220992	-0.051436	4.808194
247.390893	7982.780503	9.225997	-0.051493	4.810535
247.680640	7990.216760	9.231002	-0.051552	4.812710
247.734640	7994.708140	9.236007	-0.051565	4.814023

247.973073	7997.246545	9.241011	-0.051612	4.814764
248.143429	7998.546643	9.246016	-0.051644	4.815144
248.438552	7999.087503	9.251021	-0.051700	4.815301
248.133743	7999.932569	9.256026	-0.051644	4.815549
248.199330	7999.975301	9.261031	-0.051656	4.815561
248.665011	7999.967957	9.266035	-0.051743	4.815557
248.457152	7999.969923	9.271040	-0.051704	4.815558
248.448820	8000.001840	9.276045	-0.051703	4.815568
248.388232	7999.956016	9.281050	-0.051692	4.815555
248.670351	8000.005482	9.286055	-0.051745	4.815568
248.712728	7999.980559	9.291059	-0.051753	4.815560
248.818760	7999.957741	9.296064	-0.051773	4.815553
248.904703	7999.993331	9.301069	-0.051789	4.815563
248.854859	7999.939138	9.306074	-0.051780	4.815547
248.875920	7999.956583	9.311079	-0.051784	4.815552
249.016595	7999.968503	9.316083	-0.051810	4.815555
249.076348	7999.941727	9.321088	-0.051821	4.815547
249.321425	7999.968165	9.326093	-0.051867	4.815554
249.325955	7999.970390	9.331098	-0.051868	4.815554
249.385143	8000.015156	9.336103	-0.051880	4.815567
249.388412	8000.003477	9.341107	-0.051880	4.815564
249.274993	7999.962130	9.346112	-0.051859	4.815552
249.541001	8000.003861	9.351117	-0.051909	4.815563
249.437959	7999.939188	9.356122	-0.051890	4.815545
249.319005	7999.989591	9.361127	-0.051868	4.815560
249.435718	8000.036363	9.366131	-0.051890	4.815573
249.379056	8000.051473	9.371136	-0.051880	4.815578
249.440146	8000.062096	9.376141	-0.051891	4.815581
249.386492	8000.003568	9.381146	-0.051881	4.815564
249.409450	7999.987939	9.386151	-0.051886	4.815559
249.343151	7999.986873	9.391155	-0.051874	4.815559
249.444984	8000.003500	9.396160	-0.051893	4.815563
249.704091	8000.003470	9.401165	-0.051941	4.815562
249.543989	7999.983787	9.406170	-0.051912	4.815557
249.643457	7999.987561	9.411175	-0.051930	4.815558
249.910573	8000.012224	9.416179	-0.051980	4.815564
249.741474	7999.988122	9.421184	-0.051949	4.815557
249.825228	8000.042900	9.426189	-0.051965	4.815573
249.696951	8000.002377	9.431194	-0.051941	4.815562
249.680127	8000.012797	9.436199	-0.051938	4.815565
249.661698	8000.010376	9.441203	-0.051935	4.815564
249.823884	7999.976728	9.446208	-0.051965	4.815554
250.003600	8000.024528	9.451213	-0.051999	4.815567
249.780599	7999.996343	9.456218	-0.051957	4.815560
249.867620	8000.015933	9.461223	-0.051974	4.815565
249.970859	8000.004817	9.466227	-0.051993	4.815561
249.846011	7999.972893	9.471232	-0.051970	4.815552
249.945426	8000.021519	9.476237	-0.051989	4.815566
250.126231	8000.005262	9.481242	-0.052023	4.815561
250.057919	8000.032997	9.486247	-0.052010	4.815569
249.984828	8000.041431	9.491251	-0.051997	4.815572
250.036524	8000.011320	9.496256	-0.052006	4.815563
250.094619	8000.024030	9.501261	-0.052017	4.815566
249.980747	7999.992285	9.506266	-0.051996	4.815557
250.163801	8000.051888	9.511271	-0.052031	4.815574
250.309042	8000.069224	9.516275	-0.052058	4.815578
250.066667	8000.015092	9.521280	-0.052013	4.815564
250.073588	8000.030171	9.526285	-0.052014	4.815568
249.927846	7999.987227	9.531290	-0.051987	4.815556
250.173750	7999.964556	9.536295	-0.052033	4.815548
250.249846	8000.006394	9.541299	-0.052048	4.815560
250.174135	7999.992359	9.546304	-0.052034	4.815557
250.392687	8000.052541	9.551309	-0.052075	4.815573
250.196141	8000.025855	9.556314	-0.052038	4.815566
250.149681	8000.008025	9.561319	-0.052030	4.815561
250.267538	8000.019575	9.566323	-0.052052	4.815564
250.391829	8000.034433	9.571328	-0.052075	4.815568
250.619995	8000.049919	9.576333	-0.052118	4.815571
250.126953	8000.010919	9.581338	-0.052026	4.815562
250.369938	8000.043733	9.586343	-0.052072	4.815571
250.493204	8000.052168	9.591347	-0.052095	4.815572
250.272213	8000.026150	9.596352	-0.052054	4.815566
250.431847	8000.025567	9.601357	-0.052084	4.815565
250.400364	8000.040019	9.606362	-0.052078	4.815569
250.357377	8000.032926	9.611367	-0.052070	4.815567
250.476361	8000.022067	9.616371	-0.052093	4.815564
250.604304	8000.011355	9.621376	-0.052117	4.815560
250.538088	8000.046600	9.626381	-0.052104	4.815571
250.445862	8000.028023	9.631386	-0.052087	4.815566
250.531150	8000.033702	9.636391	-0.052103	4.815567
250.578291	8000.047302	9.641395	-0.052112	4.815571
250.506573	8000.030127	9.646400	-0.052099	4.815566
250.553217	8000.043719	9.651405	-0.052108	4.815570
250.644144	8000.017452	9.656410	-0.052125	4.815562
250.527694	8000.048673	9.661415	-0.052104	4.815571
250.681550	8000.052267	9.666419	-0.052133	4.815572
250.522110	8000.022982	9.671424	-0.052103	4.815564
250.669596	8000.057443	9.676429	-0.052131	4.815573
250.598882	8000.023197	9.681434	-0.052118	4.815563
250.824292	8000.047182	9.686439	-0.052160	4.815569
250.931357	8000.058557	9.691443	-0.052180	4.815572
250.704606	8000.001474	9.696448	-0.052138	4.815557
250.889554	8000.036546	9.701453	-0.052172	4.815566
250.832335	8000.008928	9.706458	-0.052162	4.815558
250.588885	8000.014582	9.711463	-0.052117	4.815561
250.680670	8000.020367	9.716467	-0.052134	4.815562
250.714477	8000.011323	9.721472	-0.052141	4.815559
250.757666	8000.061169	9.726477	-0.052149	4.815574
250.756470	8000.022718	9.731482	-0.052149	4.815562
250.765260	8000.043168	9.736487	-0.052151	4.815568
250.801031	8000.041631	9.741491	-0.052157	4.815568
250.680584	8000.024730	9.746496	-0.052135	4.815563
250.979492	8000.038167	9.751501	-0.052191	4.815566
251.021603	8000.014306	9.756506	-0.052199	4.815559
250.817816	8000.035559	9.761511	-0.052161	4.815566
250.694056	8000.029282	9.766515	-0.052138	4.815565
251.055747	8000.024521	9.771520	-0.052206	4.815562
251.116675	8000.043687	9.776525	-0.052217	4.815567
250.990842	8000.023493	9.781530	-0.052194	4.815562
250.969658	8000.059473	9.786535	-0.052190	4.815572
251.044100	8000.050024	9.791539	-0.052204	4.815569
250.803784	8000.029029	9.796544	-0.052160	4.815564
250.868106	8000.043978	9.801549	-0.052172	4.815568
250.922403	8000.064103	9.806554	-0.052182	4.815574
251.046724	8000.047992	9.811559	-0.052206	4.815568
251.110867	8000.024491	9.816563	-0.052218	4.815561
251.140130	8000.026052	9.821568	-0.052223	4.815562
251.204375	8000.055951	9.826573	-0.052235	4.815570
251.051630	8000.015026	9.831578	-0.052207	4.815559
251.125170	8000.061096	9.836583	-0.052221	4.815572
251.277278	8000.062527	9.841587	-0.052250	4.815572
251.117633	8000.039645	9.846592	-0.052220	4.815566
251.147170	8000.052958	9.851597	-0.052226	4.815569
251.018399	8000.026308	9.856602	-0.052202	4.815562
250.939818	8000.038924	9.861607	-0.052187	4.815566
251.040689	8000.030974	9.866611	-0.052206	4.815563
251.154947	8000.045670	9.871616	-0.052228	4.815567
251.171718	8000.060911	9.876621	-0.052231	4.815572
251.213946	8000.041324	9.881626	-0.052239	4.815566
251.213046	8000.060548	9.886631	-0.052239	4.815571
251.485248	8000.084231	9.891635	-0.052290	4.815577
251.356339	8000.067190	9.896640	-0.052266	4.815572
251.366808	8000.101551	9.901645	-0.052268	4.815582
251.442552	8000.056880	9.906650	-0.052283	4.815569
251.209219	8000.054154	9.911655	-0.052239	4.815569
251.362072	8000.052393	9.916659	-0.052268	4.815568
251.278008	8000.022201	9.921664	-0.052252	4.815560
251.441508	8000.084692	9.926669	-0.052283	4.815577
251.357437	8000.056635	9.931674	-0.052268	4.815569
251.366465	8000.061070	9.936679	-0.052269	4.815571
251.375842	8000.040946	9.941683	-0.052271	4.815565
251.281445	8000.036217	9.946688	-0.052254	4.815564
251.240034	8000.057983	9.951693	-0.052246	4.815570
251.459505	8000.042358	9.956698	-0.052287	4.815565
251.410306	8000.066134	9.961703	-0.052279	4.815572
251.443525	8000.045332	9.966707	-0.052285	4.815566
251.309904	8000.034622	9.971712	-0.052260	4.815563
251.502741	8000.061281	9.976717	-0.052296	4.815570
251.434216	8000.052702	9.981722	-0.052284	4.815568
251.445378	8000.046491	9.986727	-0.052286	4.815566
251.704519	8000.066757	9.991731	-0.052334	4.815571
251.672912	8000.049169	9.996736	-0.052329	4.815566
251.695777	8000.097617	10.001741	-0.052333	4.815580
251.608000	8000.042800	10.006746	-0.052317	4.815564
251.540021	8000.065201	10.011751	-0.052304	4.815571
251.386214	8000.065909	10.016755	-0.052276	4.815572
251.526765	8000.023364	10.021760	-0.052302	4.815559
251.770282	8000.076482	10.026765	-0.052348	4.815573
251.673539	8000.038606	10.031770	-0.052330	4.815562
251.661019	8000.061913	10.036775	-0.052328	4.815569
251.929130	8000.064170	10.041779	-0.052378	4.815569
251.738075	8000.040774	10.046784	-0.052342	4.815563
251.875823	8000.065466	10.051789	-0.052368	4.815569
251.746873	8000.037744	10.056794	-0.052344	4.815562
251.684025	8000.061297	10.061799	-0.052333	4.815569
251.782729	8000.081080	10.066803	-0.052352	4.815574
251.664494	8000.061009	10.071808	-0.052330	4.815569
251.827563	8000.089318	10.076813	-0.052360	4.815577
251.755756	8000.082821	10.081818	-0.052347	4.815575
251.500009	8000.069049	10.086823	-0.052300	4.815572
251.744974	8000.060248	10.091827	-0.052345	4.815568
251.737869	8000.025972	10.096832	-0.052344	4.815558
251.593272	8000.052462	10.101837	-0.052317	4.815567
251.658103	8000.056740	10.106842	-0.052330	4.815568
251.607051	8000.063397	10.111847	-0.052320	4.815570
251.774863	8000.061881	10.116851	-0.052352	4.815569
251.445574	8000.056519	10.121856	-0.052291	4.815569
251.490298	8000.064741	10.126861	-0.052299	4.815571
251.579073	8000.046982	10.131866	-0.052316	4.815565
251.583562	8000.060954	10.136871	-0.052317	4.815569
251.725712	8000.033387	10.141875	-0.052343	4.815561
251.632378	8000.039354	10.146880	-0.052326	4.815563
251.693845	8000.069209	10.151885	-0.052338	4.815571
251.729415	8000.043105	10.156890	-0.052345	4.815563
251.665642	8000.023924	10.161895	-0.052333	4.815558
251.731177	8000.051709	10.166899	-0.052345	4.815566
251.602205	8000.030394	10.171904	-0.052322	4.815560
251.856469	8000.066601	10.176909	-0.052369	4.815570
251.813939	8000.056310	10.181914	-0.052361	4.815567
251.590373	8000.062287	10.186919	-0.052320	4.815570
251.735835	8000.076425	10.191923	-0.052347	4.815573
251.680240	8000.048833	10.196928	-0.052337	4.815565
251.642035	8000.074924	10.201933	-0.052330	4.815573
251.675300	8000.063734	10.206938	-0.052336	4.815570
251.958534	8000.049151	10.211943	-0.052389	4.815564
251.905622	8000.070730	10.216947	-0.052380	4.815571
251.910549	8000.034514	10.221952	-0.052381	4.815560
252.001244	8000.022126	10.226957	-0.052398	4.815556
252.156559	7999.990502	10.231962	-0.052427	4.815546
251.915734	8000.010081	10.236967	-0.052382	4.815553
252.064070	8000.041354	10.241971	-0.052410	4.815561
252.251667	8000.038025	10.246976	-0.052445	4.815559
252.188385	8000.080795	10.251981	-0.052434	4.815572
251.833281	8000.055787	10.256986	-0.052368	4.815567
252.028326	8000.072871	10.261991	-0.052404	4.815571
251.974183	8000.072003	10.266995	-0.052394	4.815571
251.909602	8000.036788	10.272000	-0.052382	4.815561
252.080864	8000.074843	10.277005	-0.052414	4.815571
252.404629	8000.037426	10.282010	-0.052475	4.815558
252.038126	8000.073108	10.287015	-0.052407	4.815571
252.342352	8000.116540	10.292019	-0.052464	4.815582
252.117236	8000.078703	10.297024	-0.052422	4.815572
252.167682	8000.098766	10.302029	-0.052431	4.815577
252.128546	8000.061830	10.307034	-0.052424	4.815567
252.176215	8000.059420	10.312039	-0.052433	4.815566
252.048443	8000.069096	10.317043	-0.052410	4.815569
252.011092	8000.053550	10.322048	-0.052403	4.815565
251.967518	8000.072077	10.327053	-0.052395	4.815571
252.021373	8000.038796	10.332058	-0.052405	4.815561
252.002483	8000.033163	10.337063	-0.052402	4.815559
252.188987	8000.050108	10.342067	-0.052437	4.815563
252.005933	8000.053542	10.347072	-0.052403	4.815565
252.106366	8000.058402	10.352077	-0.052422	4.815566
252.240193	8000.058466	10.357082	-0.052447	4.815565
252.226670	8000.031561	10.362087	-0.052444	4.815557
252.236035	8000.059497	10.367091	-0.052446	4.815566
252.195772	8000.052447	10.372096	-0.052439	4.815564
252.006236	8000.066455	10.377101	-0.052404	4.815569
252.205772	8000.057981	10.382106	-0.052441	4.815565
252.340400	8000.061263	10.387111	-0.052467	4.815566
252.355098	8000.070062	10.392115	-0.052469	4.815568
252.469651	8000.037773	10.397120	-0.052491	4.815558
252.489263	8000.064808	10.402125	-0.052495	4.815566
252.316175	8000.050249	10.407130	-0.052463	4.815562
252.422854	8000.066958	10.412135	-0.052483	4.815567
252.516124	8000.082381	10.417139	-0.052500	4.815571
252.421638	8000.065901	10.422144	-0.052483	4.815567
252.527520	8000.078326	10.427149	-0.052503	4.815570
252.559156	8000.045750	10.432154	-0.052509	4.815560
252.444255	8000.090880	10.437159	-0.052488	4.815574
252.352534	8000.077650	10.442163	-0.052471	4.815570
252.456017	8000.064403	10.447168	-0.052490	4.815566
252.360704	8000.074610	10.452173	-0.052473	4.815569
252.305404	8000.074790	10.457178	-0.052462	4.815570
252.309687	8000.057787	10.462183	-0.052463	4.815565
252.417474	8000.079855	10.467187	-0.052484	4.815571
252.386422	8000.053731	10.472192	-0.052478	4.815563
252.336870	8000.088181	10.477197	-0.052469	4.815573
252.558044	8000.042681	10.482202	-0.052510	4.815559
252.368610	8000.057758	10.487207	-0.052475	4.815564
252.321143	8000.087970	10.492211	-0.052467	4.815573
252.347735	8000.082012	10.497216	-0.052472	4.815572
252.309264	8000.071787	10.502221	-0.052465	4.815569
252.266356	8000.034789	10.507226	-0.052457	4.815558
252.322423	8000.050672	10.512231	-0.052468	4.815562
252.501132	8000.079238	10.517235	-0.052501	4.815570
252.481134	8000.068247	10.522240	-0.052497	4.815567
252.434109	8000.084582	10.527245	-0.052489	4.815572
252.618855	8000.042759	10.532250	-0.052523	4.815559
252.430258	8000.072802	10.537255	-0.052488	4.815568
252.274430	8000.074544	10.542259	-0.052460	4.815570
252.497532	8000.047231	10.547264	-0.052501	4.815561
252.526863	8000.089378	10.552269	-0.052507	4.815573
252.310217	8000.071971	10.557274	-0.052467	4.815569
252.319152	8000.073200	10.562279	-0.052469	4.815569
252.495979	8000.093191	10.567283	-0.052502	4.815574
252.448748	8000.063599	10.572288	-0.052493	4.815566
252.382894	8000.062539	10.577293	-0.052481	4.815566
252.560062	8000.060108	10.582298	-0.052514	4.815564
252.390465	8000.065897	10.587303	-0.052483	4.815567
252.554400	8000.116651	10.592307	-0.052514	4.815581
252.412774	8000.050272	10.597312	-0.052487	4.815562
252.506912	8000.064641	10.602317	-0.052505	4.815566
252.638437	8000.071077	10.607322	-0.052530	4.815567
252.463594	8000.056488	10.612327	-0.052497	4.815563
252.768927	8000.052947	10.617331	-0.052554	4.815561
252.638798	8000.032680	10.622336	-0.052530	4.815556
252.583472	8000.077716	10.627341	-0.052520	4.815569
252.675320	8000.080300	10.632346	-0.052537	4.815569
252.560557	8000.078441	10.637351	-0.052516	4.815569
252.553318	8000.105038	10.642355	-0.052515	4.815577
252.443327	8000.079760	10.647360	-0.052495	4.815570
252.559238	8000.078465	10.652365	-0.052517	4.815569
252.596675	8000.057732	10.657370	-0.052524	4.815563
252.424994	8000.022903	10.662375	-0.052492	4.815554
252.501386	8000.070090	10.667379	-0.052506	4.815567
252.652065	8000.045866	10.672384	-0.052534	4.815559
252.415311	8000.077259	10.677389	-0.052491	4.815570
252.469293	8000.052524	10.682394	-0.052501	4.815562
252.638725	8000.059578	10.687399	-0.052533	4.815563
252.794508	8000.081363	10.692403	-0.052562	4.815569
252.624055	8000.062574	10.697408	-0.052530	4.815564
252.794890	8000.087808	10.702413	-0.052562	4.815571
252.703603	8000.047883	10.707418	-0.052545	4.815560
252.348743	8000.043170	10.712423	-0.052479	4.815560
252.446066	8000.075747	10.717427	-0.052498	4.815569
252.483548	8000.027247	10.722432	-0.052505	4.815555
252.454307	8000.059893	10.727437	-0.052500	4.815564
252.538030	8000.048459	10.732442	-0.052515	4.815561
252.663077	8000.056925	10.737447	-0.052539	4.815562
252.707299	8000.073683	10.742451	-0.052547	4.815567
252.502363	8000.048991	10.747456	-0.052509	4.815561
252.756859	8000.071319	10.752461	-0.052557	4.815566
252.821369	8000.077729	10.757466	-0.052569	4.815568
252.805892	8000.062539	10.762471	-0.052566	4.815563
252.744672	8000.100003	10.767475	-0.052555	4.815575
252.599731	8000.045318	10.772480	-0.052528	4.815559
252.819573	8000.073489	10.777485	-0.052569	4.815567
252.641672	8000.056714	10.782490	-0.052536	4.815562
252.514619	8000.040769	10.787495	-0.052513	4.815558
252.705798	8000.047112	10.792499	-0.052549	4.815559
252.682615	7999.995484	10.797504	-0.052545	4.815544
252.850835	8000.056988	10.802509	-0.052576	4.815562
252.770308	8000.049279	10.807514	-0.052561	4.815560
252.632858	8000.047049	10.812519	-0.052536	4.815560
252.844471	8000.076154	10.817523	-0.052575	4.815567
252.896088	8000.053516	10.822528	-0.052585	4.815560
252.919424	8000.087021	10.827533	-0.052590	4.815570
252.810570	8000.058558	10.832538	-0.052570	4.815562
252.723266	8000.048603	10.837543	-0.052554	4.815560
252.822894	8000.073742	10.842547	-0.052572	4.815567
252.793671	8000.041239	10.847552	-0.052567	4.815557
252.643431	8000.055889	10.852557	-0.052539	4.815562
252.807241	8000.067124	10.857562	-0.052570	4.815565
252.558946	8000.065219	10.862567	-0.052524	4.815565
252.594025	8000.081828	10.867571	-0.052531	4.815570
252.491306	8000.074825	10.872576	-0.052512	4.815568
252.592031	8000.101050	10.877581	-0.052531	4.815576
252.498802	8000.092066	10.882586	-0.052513	4.815573
252.645944	8000.075261	10.887591	-0.052541	4.815568
252.680642	8000.088659	10.892595	-0.052548	4.815572
252.530117	8000.109712	10.897600	-0.052520	4.815578
252.392039	8000.137376	10.902605	-0.052494	4.815587
252.612756	8000.124977	10.907610	-0.052535	4.815582
252.426240	8000.106993	10.912615	-0.052501	4.815578
252.603363	8000.087474	10.917619	-0.052534	4.815572
252.564155	8000.078304	10.922624	-0.052527	4.815569
252.644967	8000.060416	10.927629	-0.052542	4.815563
252.467886	8000.071422	10.932634	-0.052509	4.815567
252.549098	8000.058880	10.937639	-0.052525	4.815563
252.857657	8000.076752	10.942643	-0.052582	4.815567
252.606937	8000.041699	10.947648	-0.052536	4.815558
252.605408	8000.060914	10.952653	-0.052536	4.815564
252.514574	8000.063717	10.957658	-0.052519	4.815565
252.343499	8000.042782	10.962663	-0.052487	4.815560
252.374825	8000.068941	10.967667	-0.052493	4.815567
252.576842	8000.040216	10.972672	-0.052531	4.815558
252.623025	8000.095455	10.977677	-0.052540	4.815574
252.411663	8000.057841	10.982682	-0.052501	4.815564
252.477865	8000.052530	10.987687	-0.052513	4.815562
252.673085	8000.071754	10.992691	-0.052550	4.815567
252.581368	8000.049979	10.997696	-0.052533	4.815561
252.755089	8000.074192	11.002701	-0.052565	4.815567
252.825890	8000.072160	11.007706	-0.052579	4.815566
252.682191	8000.066624	11.012711	-0.052552	4.815565
252.748100	8000.084804	11.017715	-0.052564	4.815570
252.797427	8000.035429	11.022720	-0.052574	4.815555
252.592363	8000.039570	11.027725	-0.052536	4.815557
252.464873	8000.058863	11.032730	-0.052512	4.815564
252.473741	8000.049411	11.037735	-0.052514	4.815561
252.920926	8000.071684	11.042739	-0.052597	4.815565
252.643732	8000.077851	11.047744	-0.052546	4.815568
252.540582	8000.074045	11.052749	-0.052527	4.815568
252.833764	8000.076714	11.057754	-0.052582	4.815567
252.651757	8000.050260	11.062759	-0.052548	4.815560
252.634454	8000.077761	11.067763	-0.052545	4.815568
252.676356	8000.046420	11.072768	-0.052553	4.815559
252.606244	8000.079467	11.077773	-0.052540	4.815569
252.516571	8000.072677	11.082778	-0.052524	4.815567
252.629043	8000.051033	11.087783	-0.052545	4.815561
252.691887	8000.084116	11.092787	-0.052557	4.815570
252.680602	8000.054042	11.097792	-0.052555	4.815561
252.389901	8000.079213	11.102797	-0.052501	4.815570
252.498519	8000.051099	11.107802	-0.052521	4.815561
252.521383	8000.017311	11.112807	-0.052526	4.815551
252.795632	8000.069867	11.117811	-0.052577	4.815565
252.686857	8000.041405	11.122816	-0.052557	4.815557
252.848920	8000.035524	11.127821	-0.052587	4.815555
252.592186	8000.042025	11.132826	-0.052539	4.815558
252.535520	8000.043251	11.137831	-0.052529	4.815559
252.734636	8000.042247	11.142835	-0.052566	4.815557
252.665640	8000.018707	11.147840	-0.052554	4.815551
252.580857	8000.051513	11.152845	-0.052538	4.815561
252.759772	8000.058723	11.157850	-0.052571	4.815562
252.744838	8000.038202	11.162855	-0.052569	4.815556
252.825369	8000.085458	11.167859	-0.052584	4.815570
252.663317	8000.053990	11.172864	-0.052554	4.815561
252.665980	8000.073273	11.177869	-0.052555	4.815567
252.826834	8000.060964	11.182874	-0.052585	4.815562
252.468276	8000.042305	11.187879	-0.052518	4.815559
252.855935	8000.050789	11.192883	-0.052591	4.815559
252.559119	8000.034208	11.197888	-0.052536	4.815556
252.449738	8000.074089	11.202893	-0.052515	4.815568
252.590863	8000.070001	11.207898	-0.052542	4.815566
252.544814	8000.069264	11.212903	-0.052533	4.815566
252.823038	8000.086641	11.217907	-0.052585	4.815570
252.536667	8000.049938	11.222912	-0.052532	4.815561
252.515053	8000.074164	11.227917	-0.052528	4.815568
252.658928	8000.077598	11.232922	-0.052555	4.815568
252.559524	8000.051425	11.237927	-0.052537	4.815561
252.604494	8000.086351	11.242931	-0.052546	4.815571
252.644128	8000.059246	11.247936	-0.052553	4.815563
252.747914	8000.056685	11.252941	-0.052573	4.815562
252.784341	8000.062635	11.257946	-0.052580	4.815563
252.761645	8000.036647	11.262951	-0.052575	4.815556
252.766060	8000.086931	11.267955	-0.052577	4.815570
252.781787	8000.086136	11.272960	-0.052580	4.815570
252.869496	8000.081176	11.277965	-0.052596	4.815568
253.080899	8000.080373	11.282970	-0.052636	4.815567
252.657122	8000.064921	11.287975	-0.052557	4.815564
252.832654	8000.073144	11.292979	-0.052590	4.815566
253.044449	8000.034967	11.297984	-0.052629	4.815554
253.002694	8000.050320	11.302989	-0.052622	4.815558
252.978868	8000.062762	11.307994	-0.052618	4.815562
252.913909	8000.030744	11.312999	-0.052606	4.815553
252.836095	8000.056188	11.318003	-0.052591	4.815561
252.902184	8000.053011	11.323008	-0.052604	4.815560
252.935224	8000.083471	11.328013	-0.052610	4.815568
252.925465	8000.058762	11.333018	-0.052608	4.815561
252.729230	8000.063048	11.338023	-0.052572	4.815563
253.014838	8000.059185	11.343027	-0.052625	4.815561
252.774757	8000.053142	11.348032	-0.052581	4.815560
252.788546	8000.089695	11.353037	-0.052584	4.815571
252.910950	8000.059670	11.358042	-0.052607	4.815562
252.881458	8000.029299	11.363047	-0.052601	4.815553
253.040647	8000.043663	11.368051	-0.052631	4.815556
252.980662	8000.027746	11.373056	-0.052620	4.815552
253.097674	8000.071326	11.378061	-0.052642	4.815564
253.019699	8000.075407	11.383066	-0.052628	4.815566
252.871303	8000.064454	11.388071	-0.052600	4.815563
252.949675	8000.077498	11.393075	-0.052615	4.815567
252.967262	8000.039352	11.398080	-0.052618	4.815555
252.934552	8000.045241	11.403085	-0.052613	4.815557
252.924434	8000.070723	11.408090	-0.052611	4.815565
252.832474	8000.058556	11.413095	-0.052594	4.815562
252.875850	8000.062484	11.418099	-0.052602	4.815562
252.862701	8000.070829	11.423104	-0.052600	4.815565
252.843052	8000.057707	11.428109	-0.052596	4.815561
252.895477	8000.088483	11.433114	-0.052606	4.815570
252.902051	8000.038409	11.438119	-0.052608	4.815555
252.871896	8000.092401	11.443123	-0.052602	4.815571
252.961184	8000.047950	11.448128	-0.052619	4.815558
252.821830	8000.073457	11.453133	-0.052593	4.815566
252.812218	8000.081859	11.458138	-0.052592	4.815568
252.861343	8000.060249	11.463143	-0.052601	4.815562
252.931971	8000.077439	11.468147	-0.052614	4.815567
252.808339	8000.057278	11.473152	-0.052592	4.815561
252.904697	8000.066343	11.478157	-0.052610	4.815563
253.098080	8000.071654	11.483162	-0.052646	4.815564
252.958539	8000.060846	11.488167	-0.052620	4.815562
253.132304	8000.087197	11.493171	-0.052653	4.815568
252.941140	8000.057388	11.498176	-0.052617	4.815561
252.867237	8000.080760	11.503181	-0.052604	4.815568
252.804565	8000.069071	11.508186	-0.052592	4.815565
252.919661	8000.053879	11.513191	-0.052614	4.815560
253.157084	8000.066318	11.518195	-0.052658	4.815562
252.765690	8000.042850	11.523200	-0.052585	4.815557
253.002388	8000.045664	11.528205	-0.052630	4.815557
253.071037	8000.067094	11.533210	-0.052643	4.815563
252.961181	8000.063178	11.538215	-0.052622	4.815562
252.939334	8000.056428	11.543219	-0.052618	4.815560
252.828074	8000.034333	11.548224	-0.052598	4.815554
252.944735	8000.058683	11.553229	-0.052620	4.815561
253.031512	8000.065456	11.558234	-0.052636	4.815562
252.980171	8000.049681	11.563239	-0.052627	4.815558
253.101543	8000.082652	11.568243	-0.052649	4.815567
253.001806	8000.054337	11.573248	-0.052631	4.815559
253.052297	8000.061585	11.578253	-0.052641	4.815561
253.140672	8000.053432	11.583258	-0.052657	4.815558
253.090802	8000.036612	11.588263	-0.052648	4.815554
253.164283	8000.047440	11.593267	-0.052662	4.815557
252.938303	8000.069396	11.598272	-0.052620	4.815564
253.111332	8000.081851	11.603277	-0.052652	4.815567
253.039442	8000.083895	11.608282	-0.052639	4.815568
253.033957	8000.020808	11.613287	-0.052638	4.815549
252.976465	8000.071149	11.618291	-0.052628	4.815564
252.920113	8000.072380	11.623296	-0.052618	4.815565
253.001408	8000.073723	11.628301	-0.052633	4.815565
253.190053	8000.070413	11.633306	-0.052668	4.815563
252.927948	8000.017016	11.638311	-0.052620	4.815549
253.050338	8000.058548	11.643315	-0.052643	4.815560
253.271051	8000.024789	11.648320	-0.052684	4.815549
253.242383	8000.028608	11.653325	-0.052679	4.815551
253.115948	8000.083163	11.658330	-0.052655	4.815567
253.026046	8000.051804	11.663335	-0.052639	4.815558
253.245521	8000.102399	11.668339	-0.052680	4.815572
253.126443	8000.105809	11.673344	-0.052658	4.815574
252.900161	8000.087174	11.678349	-0.052616	4.815569
253.193410	8000.093049	11.683354	-0.052671	4.815570
253.017200	8000.034648	11.688359	-0.052638	4.815553
253.015017	8000.061328	11.693363	-0.052638	4.815561
252.986763	8000.051270	11.698368	-0.052633	4.815558
253.241675	8000.052246	11.703373	-0.052680	4.815557
253.192068	8000.065335	11.708378	-0.052671	4.815562
252.955801	8000.025177	11.713383	-0.052627	4.815551
253.060799	8000.020500	11.718387	-0.052647	4.815549
253.080168	8000.004811	11.723392	-0.052651	4.815544
253.063150	8000.048338	11.728397	-0.052648	4.815557
253.198410	8000.080468	11.733402	-0.052673	4.815566
253.242564	8000.026735	11.738407	-0.052682	4.815550
253.245126	8000.059901	11.743411	-0.052682	4.815560
253.064246	8000.048417	11.748416	-0.052649	4.815557
253.244149	8000.072732	11.753421	-0.052682	4.815563
253.279479	8000.092550	11.758426	-0.052689	4.815569
253.222181	8000.057452	11.763431	-0.052679	4.815559
253.225349	8000.089560	11.768435	-0.052679	4.815568
253.228996	8000.059730	11.773440	-0.052680	4.815560
253.176668	8000.071706	11.778445	-0.052671	4.815563
253.247106	8000.083553	11.783450	-0.052684	4.815567
253.131041	8000.049631	11.788455	-0.052663	4.815557
253.332103	8000.098857	11.793459	-0.052700	4.815571
253.191836	8000.041043	11.798464	-0.052674	4.815554
253.214026	8000.057441	11.803469	-0.052679	4.815559
253.488957	8000.065153	11.808474	-0.052730	4.815560
253.273164	8000.028533	11.813479	-0.052690	4.815550
253.282290	8000.072487	11.818483	-0.052692	4.815563
253.188241	8000.073101	11.823488	-0.052674	4.815564
253.028454	8000.090798	11.828493	-0.052645	4.815570
253.292030	8000.116481	11.833498	-0.052694	4.815576
253.115652	8000.061281	11.838503	-0.052661	4.815561
253.322392	8000.090307	11.843507	-0.052700	4.815568
253.266602	8000.058438	11.848512	-0.052690	4.815559
253.241413	8000.055906	11.853517	-0.052685	4.815558
253.260771	8000.073326	11.858522	-0.052689	4.815563
253.206897	8000.003039	11.863527	-0.052679	4.815543
253.064059	8000.058394	11.868531	-0.052653	4.815560
253.013306	8000.069328	11.873536	-0.052644	4.815563
253.209466	8000.029827	11.878541	-0.052680	4.815551
253.395986	8000.087360	11.883546	-0.052715	4.815567
253.299737	8000.058034	11.888551	-0.052698	4.815559
253.268142	8000.059669	11.893555	-0.052692	4.815559
253.313958	8000.070045	11.898560	-0.052701	4.815562
253.328514	8000.067094	11.903565	-0.052703	4.815561
253.368406	8000.085918	11.908570	-0.052711	4.815567
253.120575	8000.078679	11.913575	-0.052665	4.815566
253.240431	8000.088130	11.918579	-0.052688	4.815568
253.313125	8000.069040	11.923584	-0.052701	4.815562
253.132249	8000.063964	11.928589	-0.052668	4.815561
253.307508	8000.082863	11.933594	-0.052701	4.815566
253.197303	8000.028744	11.938599	-0.052680	4.815551
253.082907	8000.056795	11.943603	-0.052659	4.815559
252.966273	8000.043157	11.948608	-0.052638	4.815556
253.113195	8000.051981	11.953613	-0.052665	4.815558
253.062117	8000.081066	11.958618	-0.052656	4.815567
253.020772	8000.076134	11.963623	-0.052648	4.815565
253.164123	8000.094512	11.968627	-0.052675	4.815570
253.116690	8000.062779	11.973632	-0.052666	4.815561
253.101210	8000.063610	11.978637	-0.052664	4.815561
253.063211	8000.105725	11.983642	-0.052657	4.815574
253.060552	8000.081133	11.988647	-0.052656	4.815567
253.143186	8000.103859	11.993651	-0.052672	4.815573
253.107886	8000.078733	11.998656	-0.052666	4.815566
253.089749	8000.082724	12.003661	-0.052662	4.815567
253.329418	8000.089859	12.008666	-0.052707	4.815568
253.026307	8000.082786	12.013671	-0.052651	4.815567
253.155658	8000.074234	12.018675	-0.052675	4.815564
253.188503	8000.092943	12.023680	-0.052682	4.815569
253.048401	8000.092805	12.028685	-0.052656	4.815570
253.055790	8000.071580	12.033690	-0.052657	4.815564
253.124203	8000.048149	12.038695	-0.052670	4.815557
253.196714	8000.066438	12.043699	-0.052684	4.815562
253.197737	8000.060061	12.048704	-0.052684	4.815560
253.171071	8000.083138	12.053709	-0.052679	4.815567
253.316757	8000.093010	12.058714	-0.052707	4.815569
253.343532	8000.079578	12.063719	-0.052712	4.815565
253.378544	8000.107935	12.068723	-0.052719	4.815573
253.499811	8000.088571	12.073728	-0.052741	4.815567
253.355386	8000.065934	12.078733	-0.052715	4.815561
253.345542	8000.073264	12.083738	-0.052713	4.815563
253.334043	8000.051731	12.088743	-0.052711	4.815557
253.257932	8000.092156	12.093747	-0.052697	4.815569
253.209294	8000.082832	12.098752	-0.052688	4.815566
253.162815	8000.092768	12.103757	-0.052680	4.815569
253.465129	8000.106268	12.108762	-0.052736	4.815572
253.218850	8000.067014	12.113767	-0.052690	4.815562
253.161084	8000.090650	12.118771	-0.052680	4.815569
253.227873	8000.089620	12.123776	-0.052692	4.815568
253.340914	8000.085075	12.128781	-0.052714	4.815566
253.337245	8000.102119	12.133786	-0.052713	4.815571
253.162570	8000.069375	12.138791	-0.052681	4.815562
253.218614	8000.099143	12.143795	-0.052691	4.815571
253.275587	8000.073388	12.148800	-0.052702	4.815563
253.242337	8000.053636	12.153805	-0.052696	4.815557
253.479559	8000.086365	12.158810	-0.052740	4.815566
253.305314	8000.035471	12.163815	-0.052708	4.815552
253.361778	8000.050293	12.168819	-0.052719	4.815556
253.483094	8000.054427	12.173824	-0.052742	4.815557
253.476378	8000.081034	12.178829	-0.052741	4.815564
253.466590	8000.102250	12.183834	-0.052739	4.815571
253.478238	8000.061870	12.188839	-0.052741	4.815559
253.586500	8000.090356	12.193843	-0.052762	4.815567
253.569590	8000.087959	12.198848	-0.052759	4.815566
253.353820	8000.067359	12.203853	-0.052719	4.815561
253.563003	8000.086814	12.208858	-0.052758	4.815566
253.588622	8000.066955	12.213863	-0.052763	4.815560
253.434882	8000.108247	12.218867	-0.052734	4.815572
253.560794	8000.094300	12.223872	-0.052758	4.815568
253.477875	8000.088688	12.228877	-0.052743	4.815567
253.606279	8000.111094	12.233882	-0.052767	4.815572
253.495116	8000.053755	12.238887	-0.052746	4.815556
253.444914	8000.094603	12.243891	-0.052737	4.815568
253.438015	8000.076349	12.248896	-0.052736	4.815563
253.557927	8000.062304	12.253901	-0.052758	4.815558
253.689695	8000.118943	12.258906	-0.052783	4.815574
253.390200	8000.067069	12.263911	-0.052727	4.815561
253.576476	8000.081877	12.268915	-0.052762	4.815564
253.590677	8000.083193	12.273920	-0.052765	4.815564
253.571581	8000.076488	12.278925	-0.052762	4.815562
253.556145	8000.094408	12.283930	-0.052759	4.815568
253.556578	8000.062389	12.288935	-0.052759	4.815558
253.445554	8000.092631	12.293939	-0.052739	4.815568
253.499757	8000.072171	12.298944	-0.052749	4.815562
253.443237	8000.084079	12.303949	-0.052739	4.815565
253.590136	8000.106788	12.308954	-0.052766	4.815571
253.591747	8000.089741	12.313959	-0.052767	4.815566
253.537712	8000.110234	12.318963	-0.052757	4.815572
253.525899	8000.081219	12.323968	-0.052755	4.815564
253.747343	8000.093398	12.328973	-0.052796	4.815567
253.777303	8000.113128	12.333978	-0.052802	4.815572
253.614738	8000.093398	12.338983	-0.052772	4.815567
253.661648	8000.105928	12.343987	-0.052781	4.815571
253.596038	8000.125164	12.348992	-0.052769	4.815577
253.519174	8000.118583	12.353997	-0.052755	4.815575
253.861225	8000.156231	12.359002	-0.052819	4.815584
253.725444	8000.111305	12.364007	-0.052793	4.815572
253.775183	8000.146311	12.369011	-0.052803	4.815582
253.663410	8000.106049	12.374016	-0.052782	4.815571
253.549149	8000.095652	12.379021	-0.052761	4.815568
253.777509	8000.122897	12.384026	-0.052804	4.815575
253.502979	8000.086384	12.389031	-0.052753	4.815566
253.506038	8000.119559	12.394035	-0.052754	4.815575
253.486602	8000.090419	12.399040	-0.052750	4.815567
253.500683	8000.081052	12.404045	-0.052753	4.815564
253.414415	8000.104223	12.409050	-0.052737	4.815571
253.661823	8000.078377	12.414055	-0.052783	4.815562
253.555417	8000.099082	12.419059	-0.052764	4.815569
253.507516	8000.088702	12.424064	-0.052755	4.815566
253.594215	8000.080522	12.429069	-0.052771	4.815563
253.630331	8000.107828	12.434074	-0.052778	4.815571
253.452924	8000.069699	12.439079	-0.052745	4.815561
253.527056	8000.104035	12.444083	-0.052759	4.815571
253.533068	8000.079584	12.449088	-0.052761	4.815563
253.558480	8000.051177	12.454093	-0.052765	4.815555
253.622930	8000.089627	12.459098	-0.052778	4.815566
253.660173	8000.072095	12.464103	-0.052785	4.815561
253.718283	8000.073060	12.469107	-0.052796	4.815561
253.740949	8000.080922	12.474112	-0.052800	4.815563
253.743567	8000.083116	12.479117	-0.052801	4.815563
253.836575	8000.098536	12.484122	-0.052818	4.815567
253.593227	8000.075349	12.489127	-0.052773	4.815562
253.754272	8000.090813	12.494131	-0.052803	4.815566
253.746793	8000.088570	12.499136	-0.052802	4.815565
253.609414	8000.073524	12.504141	-0.052777	4.815561
253.718212	8000.098814	12.509146	-0.052797	4.815568
253.694019	8000.066393	12.514151	-0.052793	4.815559
253.669119	8000.093770	12.519155	-0.052788	4.815567
253.625084	8000.071705	12.524160	-0.052780	4.815561
253.546417	8000.064026	12.529165	-0.052766	4.815559
253.729052	8000.086251	12.534170	-0.052800	4.815564
253.653693	8000.061538	12.539175	-0.052786	4.815557
253.656273	8000.066936	12.544179	-0.052787	4.815559
253.737167	8000.077886	12.549184	-0.052802	4.815562
253.658118	8000.066997	12.554189	-0.052787	4.815559
253.622436	8000.090994	12.559194	-0.052781	4.815566
253.687728	8000.046150	12.564199	-0.052793	4.815553
253.850753	8000.094756	12.569203	-0.052824	4.815566
253.742423	8000.088729	12.574208	-0.052804	4.815565
253.515590	8000.040179	12.579213	-0.052762	4.815552
253.518418	8000.072281	12.584218	-0.052763	4.815561
253.502207	8000.057079	12.589223	-0.052760	4.815557
253.530764	8000.081058	12.594227	-0.052765	4.815564
253.766504	8000.073178	12.599232	-0.052809	4.815560
253.612172	8000.043970	12.604237	-0.052781	4.815552
253.714963	8000.093727	12.609242	-0.052800	4.815567
253.624567	8000.068768	12.614247	-0.052783	4.815560
253.702681	8000.080741	12.619251	-0.052798	4.815563
253.598101	8000.066230	12.624256	-0.052779	4.815559
253.526784	8000.039447	12.629261	-0.052766	4.815552
253.776251	8000.084125	12.634266	-0.052812	4.815563
253.489633	8000.073048	12.639271	-0.052759	4.815562
253.375735	8000.086154	12.644275	-0.052738	4.815566
253.675919	8000.071851	12.649280	-0.052794	4.815560
253.626880	8000.034751	12.654285	-0.052785	4.815550
253.780766	8000.074663	12.659290	-0.052814	4.815561
253.805018	8000.048374	12.664295	-0.052819	4.815553
253.674788	8000.071894	12.669299	-0.052795	4.815560
253.805479	8000.077249	12.674304	-0.052819	4.815561
253.557157	8000.052913	12.679309	-0.052773	4.815555
253.718097	8000.098281	12.684314	-0.052803	4.815568
253.718477	8000.043832	12.689319	-0.052803	4.815552
253.566987	8000.063800	12.694323	-0.052775	4.815558
253.668071	8000.069740	12.699328	-0.052794	4.815560
253.578483	8000.038386	12.704333	-0.052778	4.815551
253.635632	8000.082057	12.709338	-0.052789	4.815563
253.664005	8000.091080	12.714343	-0.052794	4.815566
253.773105	8000.097151	12.719347	-0.052815	4.815567
253.819169	8000.096851	12.724352	-0.052823	4.815567
253.667431	8000.037780	12.729357	-0.052795	4.815550
253.756794	8000.091590	12.734362	-0.052812	4.815566
253.673789	8000.065684	12.739367	-0.052797	4.815558
253.767718	8000.072574	12.744371	-0.052815	4.815560
253.753166	8000.077692	12.749376	-0.052812	4.815562
253.791681	8000.093290	12.754381	-0.052819	4.815566
253.753270	8000.095881	12.759386	-0.052812	4.815567
253.843097	8000.054643	12.764391	-0.052829	4.815554
253.699477	8000.086488	12.769395	-0.052803	4.815564
253.770319	8000.080185	12.774400	-0.052816	4.815562
253.751309	8000.063869	12.779405	-0.052813	4.815557
253.665045	8000.100924	12.784410	-0.052797	4.815569
253.701202	8000.071625	12.789415	-0.052804	4.815560
253.633762	8000.082287	12.794419	-0.052791	4.815563
253.847126	8000.075109	12.799424	-0.052831	4.815560
253.790266	8000.072059	12.804429	-0.052821	4.815560
253.781518	8000.095428	12.809434	-0.052819	4.815567
253.837663	8000.081409	12.814439	-0.052830	4.815562
254.092530	8000.095203	12.819443	-0.052878	4.815565
254.089512	8000.083420	12.824448	-0.052877	4.815562
253.858716	8000.074322	12.829453	-0.052834	4.815560
253.810737	8000.093846	12.834458	-0.052826	4.815566
253.864828	8000.075521	12.839463	-0.052836	4.815560
253.846069	8000.107271	12.844467	-0.052833	4.815570
253.867039	8000.120446	12.849472	-0.052837	4.815573
253.864081	8000.106528	12.854477	-0.052836	4.815569
253.874509	8000.115258	12.859482	-0.052838	4.815572
253.866285	8000.086302	12.864487	-0.052837	4.815563
254.032873	8000.075156	12.869491	-0.052868	4.815559
253.860735	8000.095854	12.874496	-0.052836	4.815566
253.826831	8000.083567	12.879501	-0.052830	4.815563
253.833270	8000.116797	12.884506	-0.052832	4.815572
253.908696	8000.088140	12.889511	-0.052846	4.815564
253.899761	8000.112574	12.894515	-0.052844	4.815571
254.111044	8000.093615	12.899520	-0.052884	4.815564
253.895461	8000.079425	12.904525	-0.052844	4.815561
253.997006	8000.125959	12.909530	-0.052863	4.815574
253.978037	8000.090418	12.914535	-0.052860	4.815564
254.070649	8000.106900	12.919539	-0.052877	4.815568
254.060572	8000.105683	12.924544	-0.052875	4.815568
253.888610	8000.083662	12.929549	-0.052843	4.815562
254.086196	8000.093316	12.934554	-0.052880	4.815564
254.154332	8000.096581	12.939559	-0.052893	4.815565
254.012924	8000.117782	12.944563	-0.052867	4.815572
253.909396	8000.087267	12.949568	-0.052848	4.815563
253.905812	8000.057318	12.954573	-0.052848	4.815555
254.089795	8000.091315	12.959578	-0.052882	4.815564
253.878440	8000.066514	12.964583	-0.052843	4.815557
253.862979	8000.084434	12.969587	-0.052840	4.815563
254.086713	8000.085970	12.974592	-0.052882	4.815562
253.981871	8000.063979	12.979597	-0.052863	4.815556
254.034401	8000.087282	12.984602	-0.052873	4.815563
254.118401	8000.071582	12.989607	-0.052888	4.815558
253.841724	8000.087367	12.994611	-0.052837	4.815564
254.029029	8000.092580	12.999616	-0.052872	4.815564
254.032564	8000.064884	13.004621	-0.052873	4.815556
254.001302	8000.076137	13.009626	-0.052867	4.815560
253.899686	8000.075559	13.014631	-0.052849	4.815560
253.902105	8000.089499	13.019635	-0.052849	4.815564
254.221750	8000.076583	13.024640	-0.052909	4.815559
254.022431	8000.063727	13.029645	-0.052872	4.815556
253.975054	8000.113166	13.034650	-0.052863	4.815571
253.987855	8000.080281	13.039655	-0.052866	4.815561
253.892972	8000.072337	13.044659	-0.052848	4.815559
254.063160	8000.072998	13.049664	-0.052880	4.815558
253.850698	8000.080221	13.054669	-0.052841	4.815562
253.828923	8000.090561	13.059674	-0.052837	4.815565
253.824419	8000.061665	13.064679	-0.052836	4.815556
253.892079	8000.088420	13.069683	-0.052849	4.815564
253.874664	8000.095627	13.074688	-0.052846	4.815566
253.968166	8000.067265	13.079693	-0.052864	4.815557
254.102936	8000.089777	13.084698	-0.052889	4.815563
254.097601	8000.066208	13.089703	-0.052888	4.815556
254.023021	8000.081025	13.094707	-0.052874	4.815561
254.152446	8000.095973	13.099712	-0.052899	4.815565
254.072244	8000.070111	13.104717	-0.052884	4.815557
254.152944	8000.121645	13.109722	-0.052899	4.815572
253.962734	8000.081168	13.114727	-0.052864	4.815561
254.054930	8000.111529	13.119731	-0.052881	4.815570
254.138519	8000.101162	13.124736	-0.052897	4.815566
253.970423	8000.059979	13.129741	-0.052866	4.815555
254.009795	8000.107632	13.134746	-0.052873	4.815569
254.077680	8000.092737	13.139751	-0.052886	4.815564
254.099130	8000.111260	13.144755	-0.052890	4.815569
253.932071	8000.103204	13.149760	-0.052859	4.815568
254.084362	8000.067259	13.154765	-0.052888	4.815557
254.150447	8000.087579	13.159770	-0.052900	4.815562
253.919221	8000.089155	13.164775	-0.052857	4.815564
254.198908	8000.107627	13.169779	-0.052910	4.815568
254.153769	8000.086612	13.174784	-0.052901	4.815562
254.074450	8000.070377	13.179789	-0.052887	4.815557
254.030146	8000.110255	13.184794	-0.052879	4.815569
254.187464	8000.112842	13.189799	-0.052908	4.815569
253.924464	8000.097877	13.194803	-0.052859	4.815566
253.996234	8000.110814	13.199808	-0.052873	4.815570
253.985162	8000.087151	13.204813	-0.052871	4.815563
254.172636	8000.126546	13.209818	-0.052906	4.815573
254.203281	8000.092884	13.214823	-0.052912	4.815563
254.163617	8000.109340	13.219827	-0.052905	4.815568
254.249425	8000.101146	13.224832	-0.052921	4.815566
254.263655	8000.086441	13.229837	-0.052924	4.815561
254.155026	8000.083612	13.234842	-0.052904	4.815561
254.251391	8000.090543	13.239847	-0.052922	4.815562
254.169015	8000.079599	13.244851	-0.052907	4.815560
254.052273	8000.104407	13.249856	-0.052885	4.815567
253.866969	8000.069352	13.254861	-0.052851	4.815558
254.133588	8000.108972	13.259866	-0.052901	4.815568
254.062593	8000.095009	13.264871	-0.052888	4.815565
253.946947	8000.090998	13.269875	-0.052866	4.815564
254.286744	8000.113658	13.274880	-0.052930	4.815569
254.156723	8000.062416	13.279885	-0.052906	4.815555
254.021493	8000.092263	13.284890	-0.052881	4.815564
254.207983	8000.083578	13.289895	-0.052916	4.815561
254.208060	8000.070778	13.294899	-0.052916	4.815557
254.012547	8000.108183	13.299904	-0.052879	4.815569
253.972535	8000.111817	13.304909	-0.052872	4.815570
254.113364	8000.117339	13.309914	-0.052899	4.815571
254.023499	8000.090251	13.314919	-0.052882	4.815563
253.958956	8000.111641	13.319923	-0.052870	4.815570
254.209564	8000.107209	13.324928	-0.052917	4.815567
254.097735	8000.068014	13.329933	-0.052896	4.815557
254.050976	8000.075809	13.334938	-0.052888	4.815559
254.175502	8000.053295	13.339943	-0.052911	4.815552
254.169996	8000.048948	13.344947	-0.052910	4.815551
254.221377	8000.108547	13.349952	-0.052920	4.815568
253.957977	8000.050853	13.354957	-0.052871	4.815552
254.268247	8000.096527	13.359962	-0.052929	4.815564
254.277036	8000.094550	13.364967	-0.052931	4.815563
253.956156	8000.074366	13.369971	-0.052871	4.815559
254.147680	8000.079649	13.374976	-0.052907	4.815560
254.050342	8000.069528	13.379981	-0.052889	4.815557
253.958172	8000.087262	13.384986	-0.052872	4.815563
254.184600	8000.082434	13.389991	-0.052915	4.815560
254.115551	8000.021510	13.394995	-0.052902	4.815543
254.176390	8000.088739	13.400000	-0.052913	4.815562
254.236865	8000.050225	13.405005	-0.052925	4.815551
254.389220	8000.115747	13.410010	-0.052953	4.815569
254.293166	8000.105647	13.415015	-0.052936	4.815567
253.900443	8000.109923	13.420019	-0.052863	4.815570
254.188562	8000.114648	13.425024	-0.052917	4.815570
254.060772	8000.099758	13.430029	-0.052893	4.815566
254.043600	8000.104833	13.435034	-0.052890	4.815567
254.117218	8000.091099	13.440039	-0.052904	4.815563
254.147257	8000.103354	13.445043	-0.052910	4.815567
254.359446	8000.117519	13.450048	-0.052949	4.815570
253.971367	8000.089828	13.455053	-0.052877	4.815563
254.275028	8000.100149	13.460058	-0.052934	4.815565
254.073486	8000.108617	13.465063	-0.052897	4.815568
254.050012	8000.095432	13.470067	-0.052892	4.815565
254.276909	8000.114110	13.475072	-0.052935	4.815569
253.936539	8000.078655	13.480077	-0.052872	4.815560
254.189467	8000.092418	13.485082	-0.052919	4.815563
254.018445	8000.071480	13.490087	-0.052887	4.815558
253.972483	8000.076084	13.495091	-0.052879	4.815559
254.075505	8000.082056	13.500096	-0.052898	4.815561
254.097782	8000.058938	13.505101	-0.052902	4.815554
254.144800	8000.107785	13.510106	-0.052911	4.815568
254.142691	8000.098153	13.515111	-0.052911	4.815565
254.157820	8000.096280	13.520115	-0.052914	4.815564
254.241842	8000.119030	13.525120	-0.052930	4.815571
254.254295	8000.110705	13.530125	-0.052933	4.815568
254.286601	8000.126201	13.535130	-0.052939	4.815572
254.280125	8000.099409	13.540135	-0.052938	4.815565
254.291960	8000.087869	13.545139	-0.052940	4.815561
254.473757	8000.095129	13.550144	-0.052974	4.815562
254.110457	8000.046482	13.555149	-0.052907	4.815550
254.172568	8000.109460	13.560154	-0.052918	4.815568
254.241872	8000.093520	13.565159	-0.052931	4.815563
254.130983	8000.062885	13.570163	-0.052911	4.815555
254.227595	8000.111474	13.575168	-0.052929	4.815568
254.220426	8000.095351	13.580173	-0.052928	4.815564
254.283054	8000.115616	13.585178	-0.052940	4.815569
254.130279	8000.075751	13.590183	-0.052912	4.815558
254.333969	8000.078029	13.595187	-0.052950	4.815558
254.310648	8000.088343	13.600192	-0.052945	4.815561
254.162005	8000.080588	13.605197	-0.052918	4.815560
254.318021	8000.110924	13.610202	-0.052947	4.815568
254.357456	8000.110516	13.615207	-0.052955	4.815567
254.315914	8000.094899	13.620211	-0.052947	4.815563
254.359417	8000.114851	13.625216	-0.052955	4.815569
254.175959	8000.076621	13.630221	-0.052921	4.815558
254.300250	8000.069055	13.635226	-0.052945	4.815556
254.256596	8000.095059	13.640231	-0.052937	4.815563
254.408626	8000.081539	13.645235	-0.052965	4.815559
254.357346	8000.115962	13.650240	-0.052956	4.815569
254.121632	8000.082217	13.655245	-0.052912	4.815560
254.145847	8000.089037	13.660250	-0.052917	4.815562
254.384188	8000.086541	13.665255	-0.052961	4.815560
254.467118	8000.084708	13.670259	-0.052977	4.815559
254.315092	8000.107871	13.675264	-0.052949	4.815567
254.269811	8000.090057	13.680269	-0.052941	4.815562
254.402754	8000.110403	13.685274	-0.052966	4.815567
254.362634	8000.085197	13.690279	-0.052958	4.815560
254.129143	8000.074986	13.695283	-0.052915	4.815558
254.287797	8000.092549	13.700288	-0.052945	4.815562
254.302360	8000.079985	13.705293	-0.052948	4.815559
254.350003	8000.122434	13.710298	-0.052957	4.815571
254.394143	8000.110354	13.715303	-0.052965	4.815567
254.178111	8000.089748	13.720307	-0.052925	4.815562
254.215054	8000.120274	13.725312	-0.052932	4.815571
254.478147	8000.126727	13.730317	-0.052981	4.815572
254.546994	8000.121460	13.735322	-0.052994	4.815570
254.553414	8000.122648	13.740327	-0.052996	4.815570
254.355158	8000.113013	13.745331	-0.052959	4.815568
254.318900	8000.137001	13.750336	-0.052952	4.815575
254.202726	8000.081714	13.755341	-0.052931	4.815560
254.213372	8000.118217	13.760346	-0.052933	4.815570
254.213710	8000.105421	13.765351	-0.052933	4.815567
254.238820	8000.096235	13.770355	-0.052938	4.815564
254.280407	8000.124700	13.775360	-0.052946	4.815572
254.289735	8000.073600	13.780365	-0.052948	4.815557
254.490779	8000.105741	13.785370	-0.052985	4.815565
254.312354	8000.081477	13.790375	-0.052952	4.815559
254.310968	8000.067585	13.795379	-0.052952	4.815555
254.420476	8000.106773	13.800384	-0.052973	4.815566
254.263548	8000.078589	13.805389	-0.052944	4.815558
254.283886	8000.092822	13.810394	-0.052948	4.815562
254.654651	8000.107445	13.815399	-0.053017	4.815565
254.336564	8000.068080	13.820403	-0.052958	4.815555
254.372867	8000.109276	13.825408	-0.052965	4.815567
254.287389	8000.086532	13.830413	-0.052949	4.815561
254.366655	8000.098524	13.835418	-0.052964	4.815564
254.326935	8000.093618	13.840423	-0.052957	4.815562
254.321907	8000.094619	13.845427	-0.052956	4.815563
254.610059	8000.134593	13.850432	-0.053010	4.815573
254.583871	8000.088253	13.855437	-0.053005	4.815560
254.506795	8000.105165	13.860442	-0.052991	4.815565
254.616138	8000.101628	13.865447	-0.053012	4.815563
254.461407	8000.082024	13.870451	-0.052983	4.815558
254.480038	8000.104773	13.875456	-0.052987	4.815565
254.413938	8000.106912	13.880461	-0.052974	4.815566
254.435025	8000.124361	13.885466	-0.052979	4.815571
254.518332	8000.089424	13.890471	-0.052994	4.815560
254.387515	8000.101185	13.895475	-0.052970	4.815564
254.569562	8000.111654	13.900480	-0.053004	4.815567
254.578224	8000.108607	13.905485	-0.053006	4.815566
254.322320	8000.117254	13.910490	-0.052958	4.815569
254.449579	8000.107602	13.915495	-0.052982	4.815566
254.546898	8000.081439	13.920499	-0.053001	4.815558
254.600053	8000.105821	13.925504	-0.053011	4.815565
254.447328	8000.067024	13.930509	-0.052982	4.815554
254.680983	8000.108243	13.935514	-0.053026	4.815565
254.680843	8000.105052	13.940519	-0.053026	4.815564
254.389854	8000.092832	13.945523	-0.052972	4.815562
254.422220	8000.106194	13.950528	-0.052978	4.815566
254.225109	8000.076284	13.955533	-0.052942	4.815558
254.327444	8000.106811	13.960538	-0.052961	4.815566
254.530579	8000.080242	13.965543	-0.052999	4.815557
254.610358	8000.087970	13.970547	-0.053014	4.815559
254.585492	8000.120689	13.975552	-0.053010	4.815569
254.595089	8000.089887	13.980557	-0.053012	4.815560
254.649285	8000.093993	13.985562	-0.053022	4.815561
254.504841	8000.106599	13.990567	-0.052995	4.815565
254.418738	8000.112683	13.995571	-0.052979	4.815567
254.674683	8000.125429	14.000576	-0.053027	4.815570
254.727119	8000.085715	14.005581	-0.053037	4.815558
254.738992	8000.108354	14.010586	-0.053040	4.815565
254.421443	8000.094632	14.015591	-0.052981	4.815562
254.500788	8000.091672	14.020595	-0.052996	4.815561
254.635861	8000.124871	14.025600	-0.053021	4.815570
254.427489	8000.168474	14.030605	-0.052982	4.815584
254.386845	8000.120829	14.035610	-0.052975	4.815570
254.596406	8000.129612	14.040615	-0.053014	4.815572
254.483238	8000.098938	14.045619	-0.052993	4.815563
254.493262	8000.110866	14.050624	-0.052995	4.815567
254.375730	8000.084394	14.055629	-0.052973	4.815559
254.363745	8000.097030	14.060634	-0.052971	4.815563
254.632361	8000.104643	14.065639	-0.053022	4.815564
254.474209	8000.096731	14.070643	-0.052992	4.815562
254.459111	8000.108248	14.075648	-0.052990	4.815566
254.343648	8000.081810	14.080653	-0.052968	4.815559
254.413883	8000.091518	14.085658	-0.052982	4.815561
254.512153	8000.108094	14.090663	-0.053000	4.815566
254.358709	8000.087443	14.095667	-0.052972	4.815560
254.288380	8000.115146	14.100672	-0.052959	4.815569
254.354274	8000.085265	14.105677	-0.052971	4.815560
254.382430	8000.103898	14.110682	-0.052977	4.815565
254.453115	8000.082639	14.115687	-0.052990	4.815558
254.411980	8000.077710	14.120691	-0.052982	4.815557
254.415624	8000.101282	14.125696	-0.052983	4.815564
254.285921	8000.071407	14.130701	-0.052959	4.815556
254.392050	8000.103063	14.135706	-0.052979	4.815565
254.489321	8000.113214	14.140711	-0.052998	4.815567
254.526481	8000.089271	14.145715	-0.053005	4.815560
254.432410	8000.096293	14.150720	-0.052987	4.815562
254.434407	8000.088864	14.155725	-0.052988	4.815560
254.585796	8000.093492	14.160730	-0.053016	4.815561
254.564482	8000.099567	14.165735	-0.053012	4.815563
254.621027	8000.038558	14.170739	-0.053023	4.815545
254.468350	8000.090549	14.175744	-0.052995	4.815561
254.315273	8000.077380	14.180749	-0.052967	4.815557
254.349555	8000.104658	14.185754	-0.052973	4.815565
254.420985	8000.102637	14.190759	-0.052987	4.815564
254.444328	8000.066720	14.195763	-0.052991	4.815554
254.381902	8000.059306	14.200768	-0.052980	4.815552
254.675747	8000.022471	14.205773	-0.053035	4.815540
254.639541	8000.001601	14.210778	-0.053028	4.815534
254.491302	8000.065413	14.215783	-0.053001	4.815553
254.672859	8000.073738	14.220787	-0.053035	4.815555
254.911560	8000.110768	14.225792	-0.053079	4.815564
254.661909	8000.076794	14.230797	-0.053033	4.815556
254.591599	8000.106633	14.235802	-0.053020	4.815565
254.684154	7999.248381	14.240807	-0.053037	4.815313

254.716962	7995.939457	14.245811	-0.053041	4.814346
254.585078	7990.537254	14.250816	-0.053013	4.812767
254.574616	7983.946893	14.255821	-0.053007	4.810839
254.575118	7976.596757	14.260826	-0.053002	4.808688
254.444142	7969.018661	14.265831	-0.052973	4.806470
254.497506	7961.146477	14.270835	-0.052978	4.804163
254.716861	7953.424367	14.275840	-0.053014	4.801899
254.567742	7945.348993	14.280845	-0.052981	4.799532
254.480229	7937.411580	14.285850	-0.052960	4.797204
254.498643	7929.405171	14.290855	-0.052958	4.794854
254.480815	7921.378779	14.295859	-0.052950	4.792497
254.267042	7913.339746	14.300864	-0.052905	4.790137
254.316264	7905.385983	14.305869	-0.052909	4.787798
254.209208	7897.351140	14.310874	-0.052884	4.785436
254.095425	7889.471922	14.315879	-0.052858	4.783118
254.099685	7881.414730	14.320883	-0.052854	4.780747
254.032569	7873.428422	14.325888	-0.052836	4.778395
253.915084	7865.431649	14.330893	-0.052810	4.776039
254.036137	7857.359370	14.335898	-0.052827	4.773659
253.985780	7849.405306	14.340903	-0.052813	4.771313
254.069355	7841.337337	14.345907	-0.052823	4.768932
253.933051	7833.395411	14.350912	-0.052793	4.766587
253.870524	7825.317813	14.355917	-0.052776	4.764201
253.824897	7817.427203	14.360922	-0.052763	4.761870
253.807849	7809.402536	14.365927	-0.052754	4.759497
253.601273	7801.395524	14.370931	-0.052711	4.757129
253.830773	7793.364845	14.375936	-0.052748	4.754751
253.650333	7785.300856	14.380941	-0.052710	4.752364
253.617864	7777.333218	14.385946	-0.052699	4.750003
253.592027	7769.349626	14.390951	-0.052689	4.747637
253.697708	7761.283021	14.395955	-0.052703	4.745244
253.559524	7753.369392	14.400960	-0.052673	4.742896
253.470971	7745.369831	14.405965	-0.052651	4.740522
253.331802	7737.415848	14.410970	-0.052620	4.738160
253.272999	7729.344845	14.415975	-0.052604	4.735761
253.006615	7721.277018	14.420979	-0.052550	4.733363
252.967849	7713.297372	14.425984	-0.052537	4.730990
253.042946	7705.286098	14.430989	-0.052546	4.728605
252.965418	7697.280613	14.435994	-0.052527	4.726221
252.900413	7689.275124	14.440999	-0.052510	4.723836
252.742510	7681.306416	14.446003	-0.052475	4.721462
252.654090	7673.321442	14.451008	-0.052454	4.719080
252.859674	7665.372254	14.456013	-0.052487	4.716708
252.975420	7657.289308	14.461018	-0.052503	4.714295
252.972962	7649.295225	14.466023	-0.052498	4.711907
252.646536	7641.233786	14.471027	-0.052432	4.709499
252.666687	7633.314902	14.476032	-0.052431	4.707131
252.612170	7625.306599	14.481037	-0.052416	4.704735
252.491474	7617.321748	14.486042	-0.052388	4.702346
252.475231	7609.298996	14.491047	-0.052380	4.699943
252.582809	7601.334320	14.496051	-0.052395	4.697557
252.535602	7593.243537	14.501056	-0.052381	4.695132
252.361217	7585.313306	14.506061	-0.052344	4.692754
252.518431	7577.253974	14.511066	-0.052368	4.690335
252.517354	7569.299694	14.516071	-0.052363	4.687947
252.436549	7561.264852	14.521075	-0.052343	4.685534
252.380551	7553.320527	14.526080	-0.052327	4.683146
252.310402	7545.287821	14.531085	-0.052309	4.680731
252.122004	7537.304338	14.536090	-0.052269	4.678330
252.265002	7529.294531	14.541095	-0.052291	4.675919
252.193049	7521.238037	14.546099	-0.052272	4.673493
252.211265	7513.175815	14.551104	-0.052270	4.671063
251.967109	7505.187045	14.556109	-0.052220	4.668655
251.891059	7497.208376	14.561114	-0.052201	4.666249
251.976587	7489.203475	14.566119	-0.052212	4.663833
252.040725	7481.247066	14.571123	-0.052219	4.661431
252.064984	7473.247072	14.576128	-0.052218	4.659014
251.980245	7465.280804	14.581133	-0.052197	4.656606
251.870765	7457.175152	14.586138	-0.052172	4.654155
251.904159	7449.200105	14.591143	-0.052173	4.651742
251.669438	7441.172758	14.596147	-0.052124	4.649312
251.773590	7433.266012	14.601152	-0.052139	4.646917
251.566845	7425.180250	14.606157	-0.052095	4.644467
251.613846	7417.232206	14.611162	-0.052099	4.642057
251.515212	7409.231393	14.616167	-0.052075	4.639630
251.321136	7401.253146	14.621171	-0.052034	4.637209
251.295111	7393.248594	14.626176	-0.052024	4.634778
251.429895	7385.175560	14.631181	-0.052044	4.632325
251.245946	7377.148449	14.636186	-0.052005	4.629885
251.228440	7369.187398	14.641191	-0.051997	4.627464
251.241181	7361.177222	14.646195	-0.051994	4.625026
251.334664	7353.212333	14.651200	-0.052006	4.622601
251.162630	7345.186916	14.656205	-0.051969	4.620156
251.119256	7337.168934	14.661210	-0.051956	4.617712
251.203708	7329.186962	14.666215	-0.051967	4.615278
251.062405	7321.153958	14.671219	-0.051936	4.612827
251.001713	7313.121176	14.676224	-0.051919	4.610374
250.920978	7305.178541	14.681229	-0.051899	4.607948
250.899175	7297.150217	14.686234	-0.051890	4.605495
250.863980	7289.212961	14.691239	-0.051878	4.603068
250.828793	7281.191157	14.696243	-0.051867	4.600614
250.777446	7273.198146	14.701248	-0.051852	4.598167
250.758397	7265.206314	14.706253	-0.051844	4.595719
250.830285	7257.123882	14.711258	-0.051852	4.593242
250.814829	7249.138586	14.716263	-0.051844	4.590794
250.719278	7241.087522	14.721267	-0.051821	4.588324
250.748705	7233.100559	14.726272	-0.051822	4.585873
250.689032	7225.143486	14.731277	-0.051806	4.583429
250.476447	7217.116932	14.736282	-0.051761	4.580963
250.522459	7209.151938	14.741287	-0.051764	4.578514
250.478900	7201.141742	14.746291	-0.051751	4.576051
250.237490	7193.102033	14.751296	-0.051701	4.573576
250.246880	7185.106475	14.756301	-0.051698	4.571114
250.422349	7177.071073	14.761306	-0.051726	4.568639
250.395173	7169.163245	14.766311	-0.051716	4.566201
250.275359	7161.098108	14.771315	-0.051688	4.563713
250.113318	7153.174141	14.776320	-0.051653	4.561268
250.189209	7145.138220	14.781325	-0.051662	4.558787
250.147630	7137.168816	14.786330	-0.051649	4.556325
250.137428	7129.126851	14.791335	-0.051642	4.553839
250.003462	7121.085863	14.796339	-0.051612	4.551352
250.108278	7113.101567	14.801344	-0.051627	4.548882
249.931337	7105.153316	14.806349	-0.051589	4.546421
250.107345	7097.046291	14.811354	-0.051617	4.543910
250.196722	7089.146591	14.816359	-0.051628	4.541461
249.990054	7081.151214	14.821363	-0.051585	4.538981
249.789119	7073.164284	14.826368	-0.051542	4.536503
249.792823	7065.116177	14.831373	-0.051538	4.534004
249.723134	7057.094090	14.836378	-0.051520	4.531512
249.763056	7049.102834	14.841383	-0.051522	4.529029
249.731835	7041.115438	14.846387	-0.051511	4.526545
249.837985	7033.109408	14.851392	-0.051526	4.524054
249.754254	7025.162268	14.856397	-0.051506	4.521580
249.628157	7017.073536	14.861402	-0.051477	4.519060
249.805364	7009.170327	14.866407	-0.051505	4.516598
249.576106	7001.094382	14.871411	-0.051457	4.514079
249.446442	6993.014242	14.876416	-0.051428	4.511557
249.524168	6985.037952	14.881421	-0.051437	4.509068
249.277062	6977.023813	14.886426	-0.051386	4.506564
249.219447	6969.062535	14.891431	-0.051371	4.504076
249.203242	6961.111312	14.896435	-0.051363	4.501589
249.315594	6953.092511	14.901440	-0.051378	4.499081
249.085199	6945.124167	14.906445	-0.051331	4.496586
248.964425	6937.026787	14.911450	-0.051303	4.494049
249.275875	6929.055378	14.916455	-0.051356	4.491552
249.113255	6921.012297	14.921459	-0.051321	4.489029
248.846585	6913.071339	14.926464	-0.051266	4.486537
248.814252	6905.064919	14.931469	-0.051255	4.484023
248.812847	6897.069644	14.936474	-0.051250	4.481512
248.825465	6889.064808	14.941479	-0.051247	4.478996
248.735618	6881.098326	14.946483	-0.051225	4.476491
248.796976	6873.060295	14.951488	-0.051231	4.473962
248.703398	6865.029509	14.956493	-0.051209	4.471433
248.751482	6857.026477	14.961498	-0.051213	4.468913
248.752698	6849.038392	14.966503	-0.051208	4.466395
248.770501	6840.989302	14.971507	-0.051206	4.463857
248.730586	6833.053298	14.976512	-0.051194	4.461353
248.615314	6825.045572	14.981517	-0.051167	4.458824
248.650846	6817.020828	14.986522	-0.051169	4.456290
248.502426	6809.022689	14.991527	-0.051136	4.453761
248.326814	6801.008777	14.996531	-0.051099	4.451226
248.447748	6793.000624	15.001536	-0.051116	4.448692
248.257292	6785.028663	15.006541	-0.051076	4.446168
248.119023	6776.989685	15.011546	-0.051045	4.443620
248.408065	6769.080592	15.016551	-0.051094	4.441115
248.121614	6761.012472	15.021555	-0.051035	4.438555
247.946882	6753.061673	15.026560	-0.050998	4.436031
248.202164	6745.000332	15.031565	-0.051040	4.433472
248.065616	6736.933407	15.036570	-0.051010	4.430909
247.862340	6728.979194	15.041575	-0.050967	4.428379
247.937733	6720.965685	15.046579	-0.050976	4.425831
248.050604	6712.963079	15.051584	-0.050992	4.423285
247.780579	6705.000191	15.056589	-0.050936	4.420748
247.653164	6696.981049	15.061594	-0.050908	4.418192
247.706195	6689.039210	15.066599	-0.050912	4.415660
247.847662	6680.965512	15.071603	-0.050934	4.413086
247.534528	6672.961342	15.076608	-0.050870	4.410529
247.498154	6665.001502	15.081613	-0.050859	4.407987
247.773633	6656.963099	15.086618	-0.050905	4.405420
247.749917	6649.017147	15.091623	-0.050895	4.402879
247.525774	6640.984483	15.096627	-0.050849	4.400308
247.663443	6633.000278	15.101632	-0.050869	4.397753
247.712015	6625.029972	15.106637	-0.050873	4.395201
247.318736	6616.996863	15.111642	-0.050795	4.392624
247.571872	6608.949647	15.116647	-0.050837	4.390045
247.574128	6600.956209	15.121651	-0.050832	4.387480
247.448223	6593.022217	15.126656	-0.050804	4.384932
247.252215	6585.034882	15.131661	-0.050762	4.382366
247.302139	6576.970180	15.136666	-0.050767	4.379774
247.412706	6569.042082	15.141671	-0.050782	4.377225
247.156864	6560.986646	15.146675	-0.050730	4.374631
247.165614	6552.986405	15.151680	-0.050726	4.372055
247.313002	6544.965018	15.156685	-0.050748	4.369471
247.066955	6536.992614	15.161690	-0.050698	4.366900
247.072948	6529.001774	15.166695	-0.050694	4.364322
246.944131	6521.084039	15.171699	-0.050665	4.361766
246.890464	6513.005234	15.176704	-0.050650	4.359157
246.773512	6505.035897	15.181709	-0.050623	4.356581
246.732655	6496.942387	15.186714	-0.050610	4.353963
246.785061	6488.909763	15.191719	-0.050615	4.351365
246.667115	6480.895043	15.196723	-0.050588	4.348770
246.650279	6472.907167	15.201728	-0.050580	4.346182
246.685107	6464.978840	15.206733	-0.050581	4.343613
246.516757	6456.948789	15.211738	-0.050545	4.341007
246.361842	6448.964707	15.216743	-0.050511	4.338416
246.573604	6440.971855	15.221747	-0.050545	4.335822
246.260778	6432.984464	15.226752	-0.050482	4.333225
246.286823	6424.953332	15.231757	-0.050482	4.330614
246.123348	6416.922568	15.236762	-0.050446	4.328001
246.226793	6408.985745	15.241767	-0.050461	4.325418
246.103920	6400.971478	15.246771	-0.050433	4.322807
246.182414	6392.940330	15.251776	-0.050442	4.320191
246.194806	6385.015073	15.256781	-0.050440	4.317606
246.082571	6376.932887	15.261786	-0.050414	4.314969
245.913752	6368.954519	15.266791	-0.050377	4.312363
245.992765	6360.887367	15.271795	-0.050387	4.309728
246.049654	6352.928768	15.276800	-0.050392	4.307127
246.041251	6344.919253	15.281805	-0.050386	4.304507
245.819316	6336.876815	15.286810	-0.050339	4.301874
245.879392	6328.943161	15.291815	-0.050345	4.299276
245.792895	6320.962599	15.296819	-0.050324	4.296661
245.772826	6312.917726	15.301824	-0.050316	4.294023
245.791297	6304.947260	15.306829	-0.050314	4.291408
245.723812	6296.894418	15.311834	-0.050296	4.288764
246.017806	6288.940134	15.316839	-0.050346	4.286154
245.793764	6280.945746	15.321843	-0.050299	4.283524
246.018484	6272.925961	15.326848	-0.050336	4.280889
245.675139	6264.990094	15.331853	-0.050267	4.278275
245.611642	6256.950573	15.336858	-0.050250	4.275627
245.631801	6248.924307	15.341863	-0.050249	4.272982
245.498068	6240.869179	15.346867	-0.050219	4.270326
245.450314	6232.897270	15.351872	-0.050205	4.267695
245.444085	6224.925415	15.356877	-0.050199	4.265064
245.539981	6216.907562	15.361882	-0.050212	4.262416
245.513045	6208.915918	15.366887	-0.050202	4.259775
245.343950	6200.941609	15.371891	-0.050165	4.257136
245.210596	6192.912867	15.376896	-0.050135	4.254478
245.150606	6184.896605	15.381901	-0.050119	4.251823
245.041927	6176.876374	15.386906	-0.050094	4.249165
245.231437	6168.946066	15.391911	-0.050124	4.246537
245.115544	6160.921010	15.396915	-0.050097	4.243874
244.892717	6152.946387	15.401920	-0.050051	4.241224
245.019216	6144.957474	15.406925	-0.050069	4.238572
244.955417	6136.929222	15.411930	-0.050052	4.235903
244.985137	6128.940892	15.416935	-0.050053	4.233246
244.890683	6120.875849	15.421939	-0.050030	4.230562
245.233388	6112.881877	15.426944	-0.050089	4.227903
245.047929	6104.912141	15.431949	-0.050050	4.225245
244.797679	6096.972827	15.436954	-0.049998	4.222596
244.828313	6088.955368	15.441959	-0.049999	4.219921
244.655783	6080.981823	15.446963	-0.049961	4.217257
244.721432	6072.967872	15.451968	-0.049969	4.214581
244.625504	6064.927507	15.456973	-0.049946	4.211892
244.647525	6056.953084	15.461978	-0.049945	4.209225
244.390625	6049.012841	15.466983	-0.049892	4.206565
244.448972	6040.906723	15.471987	-0.049898	4.203851
244.392203	6032.965876	15.476992	-0.049882	4.201189
244.399725	6024.935003	15.481997	-0.049878	4.198496
244.216844	6016.939494	15.487002	-0.049839	4.195811
244.358286	6008.880300	15.492007	-0.049861	4.193106
244.244696	6000.811205	15.497011	-0.049834	4.190394
244.064923	5992.885978	15.502016	-0.049796	4.187727
244.065538	5984.867261	15.507021	-0.049791	4.185030
243.986924	5976.910077	15.512026	-0.049771	4.182350
244.037968	5968.922277	15.517031	-0.049776	4.179660
243.908326	5960.955754	15.522035	-0.049747	4.176973
244.054785	5952.885320	15.527040	-0.049769	4.174253
243.790191	5944.919817	15.532045	-0.049715	4.171561
243.826255	5936.893102	15.537050	-0.049716	4.168850
243.991596	5928.906943	15.542055	-0.049742	4.166153
243.878851	5920.888276	15.547059	-0.049716	4.163440
243.732205	5912.929540	15.552064	-0.049684	4.160745
243.768499	5904.949464	15.557069	-0.049685	4.158044
243.657164	5896.909667	15.562074	-0.049660	4.155318
243.764300	5888.898901	15.567079	-0.049674	4.152603
243.533184	5880.889520	15.572083	-0.049626	4.149883
243.623021	5872.843880	15.577088	-0.049638	4.147153
243.396143	5864.866143	15.582093	-0.049591	4.144440
243.231603	5856.922729	15.587098	-0.049555	4.141737
243.389495	5848.901497	15.592103	-0.049579	4.139010
243.356768	5840.918009	15.597107	-0.049568	4.136292
243.249176	5832.886603	15.602112	-0.049543	4.133555
243.207059	5824.891154	15.607117	-0.049530	4.130829
243.291803	5816.863437	15.612122	-0.049541	4.128092
243.299857	5808.912410	15.617127	-0.049538	4.125379
243.162404	5800.924467	15.622131	-0.049507	4.122649
243.219590	5792.910919	15.627136	-0.049513	4.119911
243.330164	5784.950886	15.632141	-0.049528	4.117190
243.165106	5776.893314	15.637146	-0.049492	4.114431
243.197901	5768.902127	15.642151	-0.049493	4.111694
243.025040	5760.895802	15.647155	-0.049456	4.108949
242.871450	5752.877791	15.652160	-0.049423	4.106197
242.981275	5744.899721	15.657165	-0.049438	4.103461
242.829634	5736.893353	15.662170	-0.049405	4.100710
242.936857	5728.925121	15.667175	-0.049420	4.097974
242.587535	5720.930878	15.672179	-0.049350	4.095220
242.684231	5712.893924	15.677184	-0.049363	4.092456
242.632418	5704.891756	15.682189	-0.049348	4.089701
242.452414	5696.919990	15.687194	-0.049309	4.086952
242.354110	5688.922371	15.692199	-0.049286	4.084193
242.309377	5680.970590	15.697203	-0.049273	4.081449
242.221283	5672.937321	15.702208	-0.049251	4.078675
242.172928	5665.010050	15.707213	-0.049237	4.075935
242.278887	5656.946488	15.712218	-0.049252	4.073149
242.355409	5648.895013	15.717223	-0.049261	4.070365
242.251828	5640.930289	15.722227	-0.049237	4.067606
242.170987	5632.898011	15.727232	-0.049217	4.064823
242.239009	5624.969590	15.732237	-0.049224	4.062076
242.134560	5616.915984	15.737242	-0.049200	4.059280
242.134354	5609.004804	15.742247	-0.049195	4.056534
241.936359	5600.956294	15.747251	-0.049153	4.053736
241.967286	5592.900246	15.752256	-0.049153	4.050936
241.883235	5584.947018	15.757261	-0.049133	4.048168
241.927245	5576.932885	15.762266	-0.049136	4.045379
241.843866	5568.989711	15.767271	-0.049115	4.042611
241.735836	5560.963532	15.772275	-0.049090	4.039812
241.787680	5552.994273	15.777280	-0.049095	4.037033
241.861473	5544.958904	15.782285	-0.049104	4.034230
241.599220	5536.833735	15.787290	-0.049050	4.031388
241.650206	5528.862410	15.792295	-0.049054	4.028602
241.585191	5520.882017	15.797299	-0.049037	4.025810
241.433003	5512.897643	15.802304	-0.049004	4.023013
241.503253	5504.931371	15.807309	-0.049012	4.020224
241.487446	5496.941467	15.812314	-0.049004	4.017423
241.312323	5488.952659	15.817319	-0.048966	4.014618
241.239835	5480.914253	15.822323	-0.048947	4.011796
241.121085	5472.912048	15.827328	-0.048920	4.008983
241.214548	5464.968116	15.832333	-0.048933	4.006192
241.139564	5456.931716	15.837338	-0.048914	4.003364
241.184878	5448.956749	15.842343	-0.048917	4.000558
241.180648	5440.930262	15.847347	-0.048911	3.997731
241.047716	5432.930406	15.852352	-0.048881	3.994909
241.065946	5424.939047	15.857357	-0.048880	3.992090
241.069149	5416.892136	15.862362	-0.048875	3.989250
241.017484	5408.922418	15.867367	-0.048861	3.986434
240.955825	5400.919096	15.872371	-0.048844	3.983604
240.776826	5392.974621	15.877376	-0.048806	3.980790
240.940767	5384.984481	15.882381	-0.048831	3.977965
240.850141	5376.948523	15.887386	-0.048809	3.975116
240.777110	5368.960675	15.892391	-0.048791	3.972284
240.468041	5360.947553	15.897395	-0.048728	3.969436
240.697199	5352.962107	15.902400	-0.048766	3.966605
240.666698	5344.993834	15.907405	-0.048755	3.963773
240.627963	5336.982511	15.912410	-0.048743	3.960924
240.808357	5329.014638	15.917415	-0.048771	3.958093
240.560150	5321.008314	15.922419	-0.048720	3.955238
240.357834	5312.959223	15.927424	-0.048677	3.952367
240.461859	5304.946615	15.932429	-0.048692	3.949512
240.427951	5296.941285	15.937434	-0.048680	3.946655
240.483714	5288.974938	15.942439	-0.048686	3.943811
240.358138	5280.991846	15.947443	-0.048657	3.940956
240.190778	5273.030637	15.952448	-0.048621	3.938107
240.340428	5265.028942	15.957453	-0.048644	3.935246
240.070164	5256.992145	15.962458	-0.048589	3.932363
240.190691	5248.965246	15.967463	-0.048606	3.929489
239.860268	5241.027829	15.972467	-0.048539	3.926636
239.884758	5232.961839	15.977472	-0.048539	3.923742
240.014154	5225.005951	15.982477	-0.048558	3.920887
239.848419	5217.036999	15.987482	-0.048522	3.918019
239.932166	5209.039494	15.992487	-0.048533	3.915144
239.821418	5201.011877	15.997491	-0.048507	3.912253
239.998916	5192.958052	16.002496	-0.048535	3.909355
239.940329	5185.057409	16.007501	-0.048519	3.906506
239.575805	5176.975164	16.012506	-0.048446	3.903583
239.878735	5169.027695	16.017511	-0.048498	3.900720
239.809278	5161.021647	16.022515	-0.048480	3.897826
239.619905	5153.032199	16.027520	-0.048439	3.894934
239.594023	5145.009098	16.032525	-0.048429	3.892030
239.499261	5136.949969	16.037530	-0.048407	3.889110
239.480183	5129.048800	16.042535	-0.048398	3.886247
239.403614	5121.038634	16.047539	-0.048379	3.883341
239.418594	5113.017564	16.052544	-0.048377	3.880430
239.482580	5105.074640	16.057549	-0.048384	3.877546
239.194269	5097.021786	16.062554	-0.048325	3.874614
239.233681	5088.764381	16.067559	-0.048327	3.871611
239.261062	5080.860385	16.072563	-0.048327	3.868735
239.054995	5072.917584	16.077568	-0.048284	3.865837
239.307952	5064.959156	16.082573	-0.048326	3.862941
239.018551	5056.970490	16.087578	-0.048267	3.860020
239.121573	5049.004855	16.092583	-0.048281	3.857114
238.946056	5040.993957	16.097587	-0.048243	3.854184
238.952741	5032.985104	16.102592	-0.048239	3.851255
238.919052	5025.006766	16.107597	-0.048228	3.848335
238.824520	5016.986773	16.112602	-0.048205	3.845396
238.954702	5009.053180	16.117607	-0.048225	3.842491
238.754691	5001.042001	16.122611	-0.048182	3.839548
238.735825	4993.065094	16.127616	-0.048174	3.836620
238.616476	4985.077043	16.132621	-0.048147	3.833683
238.517409	4977.020165	16.137626	-0.048123	3.830719
238.515113	4969.054816	16.142631	-0.048118	3.827788
238.753799	4961.034327	16.147635	-0.048157	3.824840
238.607651	4953.053021	16.152640	-0.048125	3.821896
238.565135	4945.104125	16.157645	-0.048112	3.818964
238.378833	4937.075801	16.162650	-0.048072	3.815997
238.309187	4929.108728	16.167655	-0.048054	3.813053
238.438825	4921.076307	16.172659	-0.048073	3.810087
238.245095	4913.089210	16.177664	-0.048032	3.807128
238.370532	4905.104055	16.182669	-0.048050	3.804175
238.362056	4897.137974	16.187674	-0.048044	3.801223
238.263314	4889.137959	16.192679	-0.048020	3.798255
238.179688	4881.130738	16.197683	-0.048000	3.795282
237.947224	4873.102528	16.202688	-0.047952	3.792295
237.954618	4865.070673	16.207693	-0.047948	3.789310
237.761343	4857.095726	16.212698	-0.047907	3.786340
237.964715	4849.074862	16.217703	-0.047940	3.783358
238.080878	4841.097313	16.222707	-0.047956	3.780389
237.824171	4833.131726	16.227712	-0.047903	3.777413
237.872400	4825.117289	16.232717	-0.047907	3.774424
237.942420	4817.097000	16.237722	-0.047915	3.771431
237.797907	4809.097783	16.242727	-0.047883	3.768438
237.581476	4801.144426	16.247731	-0.047838	3.765458
237.416573	4793.125109	16.252736	-0.047802	3.762453
237.633691	4785.113793	16.257741	-0.047838	3.759457
237.492928	4777.180779	16.262746	-0.047807	3.756479
237.622246	4769.127635	16.267751	-0.047826	3.753461
237.602760	4761.088486	16.272755	-0.047817	3.750441
237.194279	4753.124873	16.277760	-0.047736	3.747439
237.208446	4745.111574	16.282765	-0.047733	3.744425
237.291391	4737.155966	16.287770	-0.047744	3.741432
237.324150	4729.130322	16.292775	-0.047745	3.738410
237.091681	4721.185808	16.297779	-0.047697	3.735409
237.068625	4713.148541	16.302784	-0.047687	3.732375
237.339343	4705.130604	16.307789	-0.047733	3.729354
236.868402	4697.190152	16.312794	-0.047640	3.726342
236.981509	4689.180311	16.317799	-0.047656	3.723314
237.154871	4681.178032	16.322803	-0.047683	3.720289
237.091037	4673.227062	16.327808	-0.047666	3.717275
236.964786	4665.242149	16.332813	-0.047638	3.714244
237.061234	4657.096489	16.337818	-0.047650	3.711156
236.971602	4649.098618	16.342823	-0.047629	3.708116
236.927963	4641.156084	16.347827	-0.047616	3.705095
236.753281	4633.183470	16.352832	-0.047578	3.702058
236.708265	4625.215569	16.357837	-0.047565	3.699023
236.504082	4617.235998	16.362842	-0.047522	3.695977
236.684070	4609.211672	16.367847	-0.047550	3.692921
236.801847	4601.199650	16.372851	-0.047567	3.689866
236.500310	4593.212945	16.377856	-0.047506	3.686808
236.453210	4585.234099	16.382861	-0.047492	3.683756
236.612016	4577.266144	16.387866	-0.047517	3.680711
236.606424	4569.261897	16.392871	-0.047510	3.677645
236.475020	4561.282515	16.397875	-0.047481	3.674584
236.354441	4553.248922	16.402880	-0.047453	3.671499
236.419387	4545.248679	16.407885	-0.047461	3.668429
236.393508	4537.254738	16.412890	-0.047451	3.665357
236.310173	4529.261665	16.417895	-0.047430	3.662281
236.199848	4521.262588	16.422899	-0.047405	3.659199
236.050129	4513.306197	16.427904	-0.047372	3.656130
235.891585	4505.311024	16.432909	-0.047337	3.653043
236.072695	4497.221004	16.437914	-0.047366	3.649926
236.055374	4489.274252	16.442919	-0.047357	3.646857
235.923275	4481.268633	16.447923	-0.047328	3.643759
235.702797	4473.311477	16.452928	-0.047282	3.640674
235.972499	4465.321611	16.457933	-0.047327	3.637588
235.671706	4457.316792	16.462938	-0.047266	3.634478
235.487861	4449.260140	16.467943	-0.047227	3.631348
235.534409	4441.291718	16.472947	-0.047230	3.628256
235.597900	4433.258206	16.477952	-0.047237	3.625137
235.760503	4425.298464	16.482957	-0.047262	3.622046
235.543416	4417.308013	16.487962	-0.047217	3.618930
235.542445	4409.353364	16.492967	-0.047212	3.615831
235.377517	4401.363506	16.497971	-0.047176	3.612712
235.143154	4393.331172	16.502976	-0.047127	3.609571
235.428110	4385.354502	16.507981	-0.047175	3.606464
235.087552	4377.348559	16.512986	-0.047107	3.603325
235.190833	4369.369062	16.517991	-0.047121	3.600206
235.269498	4361.423708	16.522995	-0.047131	3.597097
235.295809	4353.383847	16.528000	-0.047130	3.593947
235.282530	4345.375364	16.533005	-0.047123	3.590805
235.212694	4337.365270	16.538010	-0.047105	3.587659
235.021503	4329.401215	16.543015	-0.047064	3.584524
234.998519	4321.455799	16.548019	-0.047055	3.581399
234.839243	4313.415483	16.553024	-0.047020	3.578229
234.929198	4305.425942	16.558029	-0.047032	3.575084
234.722988	4297.404153	16.563034	-0.046989	3.571915
234.531818	4289.419315	16.568039	-0.046948	3.568758
234.604045	4281.441987	16.573043	-0.046956	3.565609
234.475658	4273.446238	16.578048	-0.046927	3.562444
234.492722	4265.443737	16.583053	-0.046926	3.559277
234.493270	4257.474004	16.588058	-0.046921	3.556121
234.521598	4249.404593	16.593063	-0.046921	3.552922
234.258422	4241.363402	16.598067	-0.046867	3.549724
234.324736	4233.376439	16.603072	-0.046874	3.546554
234.542622	4225.422909	16.608077	-0.046910	3.543399
234.350438	4217.450726	16.613082	-0.046869	3.540221
234.337383	4209.475426	16.618087	-0.046861	3.537045
234.382752	4201.447299	16.623091	-0.046865	3.533846
234.239559	4193.437581	16.628096	-0.046833	3.530647
234.310619	4185.472064	16.633101	-0.046841	3.527468
234.073377	4177.446603	16.638106	-0.046792	3.524253
234.053435	4169.507939	16.643111	-0.046783	3.521077
233.947197	4161.486414	16.648115	-0.046758	3.517862
233.821550	4153.508805	16.653120	-0.046730	3.514661
233.954396	4145.532645	16.658125	-0.046750	3.511466
233.871695	4137.493262	16.663130	-0.046729	3.508235
233.933666	4129.489744	16.668135	-0.046736	3.505021
233.947630	4121.526746	16.673139	-0.046733	3.501818
233.748175	4113.528705	16.678144	-0.046691	3.498592
233.966253	4105.565245	16.683149	-0.046727	3.495390
233.825962	4097.579717	16.688154	-0.046696	3.492164
233.747154	4089.580592	16.693159	-0.046676	3.488933
233.714639	4081.603821	16.698163	-0.046665	3.485708
233.594760	4073.617405	16.703168	-0.046638	3.482474
233.605536	4065.637416	16.708173	-0.046634	3.479244
233.541071	4057.634591	16.713178	-0.046617	3.475999
233.278861	4049.631863	16.718183	-0.046564	3.472744
233.082104	4041.611580	16.723187	-0.046522	3.469482
233.227838	4033.598540	16.728192	-0.046544	3.466230
233.456728	4025.622377	16.733197	-0.046582	3.462993
233.143909	4017.640196	16.738202	-0.046518	3.459733
233.231029	4009.659645	16.743207	-0.046530	3.456484
233.280808	4001.621480	16.748211	-0.046534	3.453207
233.128344	3993.603405	16.753216	-0.046500	3.449928
232.972045	3985.685727	16.758221	-0.046466	3.446687
232.934175	3977.666815	16.763226	-0.046454	3.443406
233.061926	3969.687089	16.768231	-0.046473	3.440143
232.899904	3961.720184	16.773235	-0.046438	3.436872
233.084436	3953.670304	16.778240	-0.046467	3.433576
232.877508	3945.681354	16.783245	-0.046423	3.430288
232.616716	3937.707614	16.788250	-0.046370	3.427002
232.467315	3929.720363	16.793255	-0.046337	3.423711
232.750555	3921.709792	16.798259	-0.046385	3.420421
232.623420	3913.715686	16.803264	-0.046356	3.417122
232.679438	3905.751271	16.808269	-0.046361	3.413837
232.629492	3897.724709	16.813274	-0.046347	3.410521
232.467051	3889.765149	16.818279	-0.046312	3.407224
232.504214	3881.761304	16.823283	-0.046314	3.403914
232.350459	3873.797746	16.828288	-0.046280	3.400610
232.557546	3865.823096	16.833293	-0.046314	3.397310
232.362039	3857.804909	16.838298	-0.046272	3.393976
232.334446	3849.709227	16.843303	-0.046262	3.390611
232.261770	3841.769466	16.848307	-0.046243	3.387307
232.152762	3833.783587	16.853312	-0.046218	3.383979
232.100294	3825.856251	16.858317	-0.046203	3.380674
232.218429	3817.831694	16.863322	-0.046220	3.377331
232.234487	3809.824458	16.868327	-0.046218	3.373989
232.030281	3801.843927	16.873331	-0.046175	3.370646
232.051669	3793.833492	16.878336	-0.046174	3.367296
232.048687	3785.869625	16.883341	-0.046168	3.363961
231.853577	3777.895157	16.888346	-0.046127	3.360612
231.812078	3769.925194	16.893351	-0.046114	3.357266
231.932282	3761.900968	16.898355	-0.046132	3.353900
231.955962	3753.856715	16.903360	-0.046131	3.350519
231.769189	3745.918133	16.908365	-0.046091	3.347171
231.681562	3737.901206	16.913370	-0.046070	3.343791
231.671935	3729.941886	16.918375	-0.046063	3.340434
231.601635	3721.959642	16.923379	-0.046045	3.337062
231.441102	3713.956462	16.928384	-0.046010	3.333674
231.500111	3705.945966	16.933389	-0.046016	3.330288
231.361605	3697.959450	16.938394	-0.045985	3.326902
231.382338	3689.971549	16.943399	-0.045984	3.323517
231.261698	3682.015272	16.948403	-0.045956	3.320137
231.245930	3674.021895	16.953408	-0.045948	3.316741
231.209393	3666.041490	16.958413	-0.045937	3.313347
230.913462	3657.994780	16.963418	-0.045876	3.309911
230.937457	3650.025540	16.968423	-0.045876	3.306517
230.841893	3642.053178	16.973427	-0.045853	3.303113
230.841618	3634.049145	16.978432	-0.045848	3.299696
230.909017	3626.074366	16.983437	-0.045856	3.296291
230.899086	3618.044713	16.988442	-0.045849	3.292855
230.881714	3610.045247	16.993447	-0.045840	3.289429
230.864797	3602.095577	16.998451	-0.045832	3.286020
230.728244	3594.112611	17.003456	-0.045802	3.282589
230.749021	3586.141990	17.008461	-0.045801	3.279166
230.687537	3578.155941	17.013466	-0.045784	3.275729
230.751683	3570.114707	17.018471	-0.045791	3.272270
230.536928	3562.139195	17.023475	-0.045746	3.268825
230.210433	3554.172266	17.028480	-0.045680	3.265375
230.294523	3546.196615	17.033485	-0.045691	3.261934
230.206802	3538.176514	17.038490	-0.045669	3.258463
230.096258	3530.195218	17.043495	-0.045644	3.255004
230.254953	3522.199134	17.048499	-0.045668	3.251546
230.042985	3514.190975	17.053504	-0.045624	3.248065
230.098342	3506.220713	17.058509	-0.045629	3.244607
229.942935	3498.272693	17.063514	-0.045595	3.241146
229.961893	3490.297703	17.068519	-0.045594	3.237677
230.011051	3482.264690	17.073523	-0.045598	3.234180
229.915401	3474.182275	17.078528	-0.045575	3.230651
229.929474	3466.210722	17.083533	-0.045572	3.227172
229.876871	3458.209728	17.088538	-0.045558	3.223674
229.589145	3450.281570	17.093543	-0.045499	3.220194
229.572879	3442.318104	17.098547	-0.045491	3.216705
229.519684	3434.299150	17.103552	-0.045476	3.213188
229.585954	3426.309731	17.108557	-0.045483	3.209684
229.557174	3418.313846	17.113562	-0.045473	3.206169
229.616672	3410.305616	17.118567	-0.045479	3.202649
229.522506	3402.368221	17.123571	-0.045456	3.199150
229.432403	3394.407321	17.128576	-0.045435	3.195637
229.183400	3386.403902	17.133581	-0.045383	3.192094
229.193738	3378.369197	17.138586	-0.045380	3.188545
229.386637	3370.383818	17.143591	-0.045411	3.185021
229.249798	3362.445134	17.148595	-0.045381	3.181500
229.271227	3354.430423	17.153600	-0.045379	3.177948
229.215983	3346.458058	17.158605	-0.045364	3.174408
229.094471	3338.466594	17.163610	-0.045337	3.170852
229.151180	3330.454308	17.168615	-0.045342	3.167291
229.044095	3322.480181	17.173619	-0.045317	3.163736
229.053061	3314.493315	17.178624	-0.045314	3.160176
229.028205	3306.521532	17.183629	-0.045304	3.156617
228.693118	3298.539388	17.188634	-0.045237	3.153036
228.808156	3290.471629	17.193639	-0.045253	3.149432
228.650854	3282.540712	17.198643	-0.045219	3.145874
228.787743	3274.509987	17.203648	-0.045239	3.142279
228.436180	3266.609332	17.208653	-0.045169	3.138718
228.241240	3258.608673	17.213658	-0.045127	3.135114
228.433626	3250.590236	17.218663	-0.045158	3.131515
228.367180	3242.607176	17.223667	-0.045141	3.127917
228.403254	3234.585135	17.228672	-0.045142	3.124301
228.334138	3226.668499	17.233677	-0.045125	3.120725
228.230225	3218.686420	17.238682	-0.045100	3.117112
228.344536	3210.661587	17.243687	-0.045116	3.113486
228.399250	3202.650613	17.248691	-0.045122	3.109860
228.299860	3194.678802	17.253696	-0.045098	3.106240
228.223609	3186.712645	17.258701	-0.045079	3.102619
228.079798	3178.737209	17.263706	-0.045047	3.098987
228.078941	3170.749976	17.268711	-0.045042	3.095352
228.039441	3162.747945	17.273715	-0.045029	3.091704
227.844904	3154.774440	17.278720	-0.044988	3.088057
227.741855	3146.792326	17.283725	-0.044964	3.084407
227.826984	3138.811578	17.288730	-0.044975	3.080761
227.758020	3130.844284	17.293735	-0.044957	3.077110
227.706239	3122.825515	17.298739	-0.044942	3.073432
227.437948	3114.763639	17.303744	-0.044887	3.069720
227.422262	3106.814218	17.308749	-0.044879	3.066067
227.385380	3098.849997	17.313754	-0.044867	3.062401
227.314623	3090.878479	17.318759	-0.044849	3.058726
227.454769	3082.882759	17.323763	-0.044870	3.055046
227.292602	3074.889840	17.328768	-0.044835	3.051348
227.370456	3066.906947	17.333773	-0.044844	3.047661
227.363311	3058.919525	17.338778	-0.044838	3.043964
227.177632	3050.960271	17.343783	-0.044799	3.040267
227.154305	3043.008100	17.348787	-0.044789	3.036577
226.914370	3034.996069	17.353792	-0.044739	3.032843
227.270817	3026.968250	17.358797	-0.044801	3.029127
227.020138	3019.009319	17.363802	-0.044749	3.025409
226.895826	3011.054477	17.368807	-0.044721	3.021694
227.134964	3003.046756	17.373811	-0.044760	3.017967
226.804997	2995.069026	17.378816	-0.044694	3.014222
226.923745	2987.048964	17.383821	-0.044711	3.010475
226.848094	2979.098551	17.388826	-0.044692	3.006746
226.710545	2971.130642	17.393831	-0.044661	3.003001
226.453964	2963.181318	17.398835	-0.044608	2.999255
226.482141	2955.192059	17.403840	-0.044609	2.995498
226.578615	2947.151247	17.408845	-0.044622	2.991717
226.501725	2939.158134	17.413850	-0.044602	2.987944
226.428674	2931.160871	17.418855	-0.044584	2.984165
226.612033	2923.206540	17.423859	-0.044613	2.980414
226.396418	2915.244697	17.428864	-0.044568	2.976635
226.351839	2907.249126	17.433869	-0.044554	2.972844
226.246136	2899.239420	17.438874	-0.044530	2.969038
226.276119	2891.258322	17.443879	-0.044530	2.965247
226.208710	2883.318209	17.448883	-0.044513	2.961466
226.171588	2875.325407	17.453888	-0.044501	2.957657
226.157133	2867.360756	17.458893	-0.044493	2.953858
225.976930	2859.356322	17.463898	-0.044454	2.950026
225.940246	2851.357945	17.468903	-0.044442	2.946199
226.198734	2843.383594	17.473907	-0.044486	2.942394
226.035644	2835.407286	17.478912	-0.044450	2.938562
225.882907	2827.444895	17.483917	-0.044417	2.934732
225.835389	2819.443218	17.488922	-0.044403	2.930883
225.881882	2811.460612	17.493927	-0.044406	2.927043
225.649120	2803.509935	17.498931	-0.044358	2.923199
225.611511	2795.506437	17.503936	-0.044346	2.919334
225.784891	2787.543987	17.508941	-0.044373	2.915496
225.689316	2779.469980	17.513946	-0.044350	2.911584
225.377044	2771.496421	17.518951	-0.044287	2.907704
225.630618	2763.511108	17.523955	-0.044329	2.903843
225.335059	2755.582846	17.528960	-0.044269	2.899976
225.413872	2747.610399	17.533965	-0.044279	2.896102
225.292302	2739.627892	17.538970	-0.044251	2.892207
225.410667	2731.597564	17.543975	-0.044268	2.888296
225.246631	2723.659940	17.548979	-0.044233	2.884410
224.988885	2715.714206	17.553984	-0.044180	2.880510
225.278219	2707.729100	17.558989	-0.044229	2.876615
225.112018	2699.728645	17.563994	-0.044193	2.872682
225.054146	2691.735989	17.568999	-0.044177	2.868754
225.203170	2683.733622	17.574003	-0.044200	2.864826
224.980951	2675.794666	17.579008	-0.044153	2.860905
224.919651	2667.823282	17.584013	-0.044137	2.856970
224.974584	2659.832106	17.589018	-0.044142	2.853027
224.934264	2651.809718	17.594023	-0.044129	2.849058
224.960757	2643.852708	17.599027	-0.044129	2.845119
224.718778	2635.930861	17.604032	-0.044079	2.841177
224.789939	2627.958802	17.609037	-0.044088	2.837223
224.563552	2619.968315	17.614042	-0.044040	2.833236
224.536432	2611.932022	17.619047	-0.044030	2.829233
224.591574	2603.978428	17.624051	-0.044035	2.825270
224.490975	2596.000051	17.629056	-0.044012	2.821280
224.534393	2588.012769	17.634061	-0.044015	2.817288
224.403928	2580.049264	17.639066	-0.043985	2.813293
224.401980	2572.029492	17.644071	-0.043980	2.809271
224.202349	2564.104224	17.649075	-0.043938	2.805279
224.162833	2556.129076	17.654080	-0.043926	2.801266
224.227580	2548.155808	17.659085	-0.043933	2.797253
224.060391	2540.183056	17.664090	-0.043896	2.793222
223.987063	2532.175202	17.669095	-0.043878	2.789173
224.270549	2524.191854	17.674099	-0.043925	2.785151
224.235019	2516.223114	17.679104	-0.043914	2.781112
224.004921	2508.297245	17.684109	-0.043866	2.777078
223.969396	2500.289701	17.689114	-0.043854	2.773007
223.981211	2492.282267	17.694119	-0.043851	2.768934
223.770662	2484.354888	17.699123	-0.043807	2.764882
223.545849	2476.393846	17.704128	-0.043760	2.760806
223.654042	2468.417775	17.709133	-0.043776	2.756736
223.548534	2460.397500	17.714138	-0.043751	2.752624
223.431997	2452.361962	17.719143	-0.043724	2.748498
223.411258	2444.403811	17.724147	-0.043715	2.744412
223.439873	2436.431665	17.729152	-0.043716	2.740315
223.203160	2428.502242	17.734157	-0.043666	2.736217
223.390277	2420.469818	17.739162	-0.043696	2.732087
223.336268	2412.496207	17.744167	-0.043681	2.727965
223.478101	2404.519809	17.749171	-0.043703	2.723848
223.240607	2396.581335	17.754176	-0.043653	2.719721
223.350900	2388.626747	17.759181	-0.043669	2.715601
223.162853	2380.632789	17.764186	-0.043629	2.711436
222.969600	2372.666830	17.769191	-0.043588	2.707278
223.150315	2364.689296	17.774195	-0.043616	2.703132
222.986167	2356.723506	17.779200	-0.043581	2.698963
222.870420	2348.791736	17.784205	-0.043554	2.694809
222.747010	2340.788586	17.789210	-0.043526	2.690611
222.850165	2332.784915	17.794215	-0.043540	2.686420
222.784923	2324.862142	17.799219	-0.043523	2.682254
222.534787	2316.882791	17.804224	-0.043472	2.678040
222.485434	2308.933814	17.809229	-0.043457	2.673849
222.485259	2300.871358	17.814234	-0.043452	2.669594
222.530115	2292.892402	17.819239	-0.043456	2.665379
222.346158	2284.965125	17.824243	-0.043416	2.661170
222.270720	2277.006063	17.829248	-0.043397	2.656945
222.447979	2268.990623	17.834253	-0.043425	2.652699
222.366286	2261.029887	17.839258	-0.043405	2.648459
222.300652	2253.054213	17.844263	-0.043388	2.644205
222.276514	2245.109399	17.849267	-0.043378	2.639964
222.030822	2237.177782	17.854272	-0.043328	2.635708
221.977257	2229.182126	17.859277	-0.043313	2.631423
222.080995	2221.169049	17.864282	-0.043327	2.627133
221.796499	2213.231225	17.869287	-0.043269	2.622850
221.821855	2205.277146	17.874291	-0.043269	2.618572
221.800593	2197.288867	17.879296	-0.043260	2.614266
221.660699	2189.309713	17.884301	-0.043229	2.609949
221.474455	2181.354797	17.889306	-0.043189	2.605635
221.496987	2173.383979	17.894311	-0.043188	2.601320
221.570644	2165.425165	17.899315	-0.043197	2.597007
221.490934	2157.339400	17.904320	-0.043177	2.592607
221.395200	2149.288319	17.909325	-0.043154	2.588218
221.348893	2141.359737	17.914330	-0.043140	2.583892
221.130468	2133.444652	17.919335	-0.043095	2.579554
221.239876	2125.495792	17.924339	-0.043110	2.575213
221.127449	2117.513642	17.929344	-0.043084	2.570831
221.227275	2109.555608	17.934349	-0.043098	2.566469
221.117429	2101.621644	17.939354	-0.043072	2.562098
221.158422	2093.653596	17.944359	-0.043075	2.557712
221.261820	2085.677994	17.949363	-0.043089	2.553318
220.965588	2077.725009	17.954368	-0.043029	2.548902
220.905895	2069.758452	17.959373	-0.043013	2.544486
220.955095	2061.803420	17.964378	-0.043017	2.540078
220.742535	2053.859326	17.969383	-0.042972	2.535649
220.672571	2045.885810	17.974387	-0.042954	2.531205
220.644210	2037.897516	17.979392	-0.042944	2.526749
220.750078	2029.934614	17.984397	-0.042959	2.522309
220.578300	2022.008174	17.989402	-0.042922	2.517861
220.558357	2014.009839	17.994407	-0.042913	2.513376
220.681911	2005.993995	17.999411	-0.042931	2.508884
220.380211	1998.046105	18.004416	-0.042870	2.504391
220.503299	1990.096036	18.009421	-0.042888	2.499920
220.535238	1982.132661	18.014426	-0.042889	2.495426
220.363596	1974.167211	18.019431	-0.042852	2.490908
220.376913	1966.209680	18.024435	-0.042849	2.486400
220.348467	1958.245337	18.029440	-0.042839	2.481877
220.363875	1950.296678	18.034445	-0.042837	2.477358
220.012083	1942.364323	18.039450	-0.042766	2.472812
219.919281	1934.373656	18.044455	-0.042744	2.468244
220.230731	1926.379956	18.049459	-0.042797	2.463696
219.984792	1918.451650	18.054464	-0.042746	2.459136
219.798202	1910.512766	18.059469	-0.042706	2.454565
219.832308	1902.521596	18.064474	-0.042708	2.449972
219.726202	1894.567045	18.069479	-0.042683	2.445381
219.845678	1886.608627	18.074483	-0.042700	2.440796
219.734848	1878.656582	18.079488	-0.042674	2.436189
219.756295	1870.636787	18.084493	-0.042673	2.431544
219.381733	1862.690253	18.089498	-0.042599	2.426902
219.371313	1854.718215	18.094503	-0.042592	2.422265
219.663951	1846.747247	18.099507	-0.042641	2.417642
219.526817	1838.795468	18.104512	-0.042611	2.412989
219.520921	1830.825672	18.109517	-0.042604	2.408326
219.333461	1822.903449	18.114522	-0.042564	2.403668
219.290363	1814.956211	18.119527	-0.042551	2.398998
219.159107	1807.031728	18.124531	-0.042522	2.394325
219.052654	1799.034305	18.129536	-0.042497	2.389601
219.225418	1791.053134	18.134541	-0.042524	2.384900
219.037709	1783.127198	18.139546	-0.042484	2.380194
218.895458	1775.185443	18.144551	-0.042453	2.375472
218.955908	1767.219718	18.149555	-0.042459	2.370744
218.691172	1759.264898	18.154560	-0.042405	2.365986
218.487487	1751.352774	18.159565	-0.042362	2.361248
218.653827	1743.373053	18.164570	-0.042388	2.356491
218.638222	1735.362859	18.169575	-0.042380	2.351691
218.587495	1727.402347	18.174579	-0.042365	2.346908
218.463921	1719.453444	18.179584	-0.042337	2.342117
218.502671	1711.512552	18.184589	-0.042340	2.337334
218.504106	1703.544155	18.189594	-0.042335	2.332521
218.442947	1695.562325	18.194599	-0.042318	2.327685
218.425816	1687.636360	18.199603	-0.042310	2.322877
218.355000	1679.696677	18.204608	-0.042292	2.318045
218.253885	1671.761081	18.209613	-0.042268	2.313204
218.352536	1663.764216	18.214618	-0.042282	2.308331
218.051037	1655.848962	18.219623	-0.042221	2.303465
217.988889	1647.925395	18.224627	-0.042204	2.298604
218.015469	1639.935844	18.229632	-0.042204	2.293699
217.864500	1631.999704	18.234637	-0.042171	2.288801
218.005317	1624.014373	18.239642	-0.042192	2.283887
217.676783	1616.113443	18.244647	-0.042126	2.278975
217.712156	1608.156791	18.249651	-0.042127	2.274049
217.558272	1600.125508	18.254656	-0.042094	2.269049
217.591220	1592.172818	18.259661	-0.042095	2.264104
217.607046	1584.232094	18.264666	-0.042093	2.259153
217.535307	1576.286743	18.269671	-0.042074	2.254182
217.534305	1568.340894	18.274675	-0.042069	2.249205
217.305075	1560.398980	18.279680	-0.042021	2.244199
217.392112	1552.479601	18.284685	-0.042033	2.239224
217.410814	1544.532896	18.289690	-0.042031	2.234215
217.188963	1536.571044	18.294695	-0.041985	2.229164
217.264191	1528.619950	18.299699	-0.041994	2.224134
217.094289	1520.696376	18.304704	-0.041957	2.219089
216.952068	1512.768167	18.309709	-0.041926	2.214032
216.850626	1504.813544	18.314714	-0.041902	2.208950
216.790358	1496.854406	18.319719	-0.041886	2.203857
216.801182	1488.935295	18.324723	-0.041883	2.198784
216.603722	1480.988607	18.329728	-0.041841	2.193663
216.755693	1472.982565	18.334733	-0.041864	2.188523
216.715956	1465.048228	18.339738	-0.041852	2.183400
216.371546	1457.154787	18.344743	-0.041783	2.178264
216.432999	1449.202076	18.349747	-0.041789	2.173114
216.457410	1441.233356	18.354752	-0.041789	2.167938
216.390610	1433.299020	18.359757	-0.041771	2.162764
216.348953	1425.381787	18.364762	-0.041758	2.157591
216.279021	1417.436615	18.369767	-0.041740	2.152384
216.391501	1409.470820	18.374771	-0.041756	2.147169
216.134584	1401.557758	18.379776	-0.041704	2.141940
215.976976	1393.654670	18.384781	-0.041669	2.136715
216.003891	1385.696619	18.389786	-0.041669	2.131458
215.823578	1377.746082	18.394791	-0.041631	2.126173
215.869519	1369.816406	18.399795	-0.041634	2.120911
215.683823	1361.899255	18.404800	-0.041595	2.115621
215.729606	1353.887553	18.409805	-0.041598	2.110278
215.621116	1345.963123	18.414810	-0.041573	2.104964
215.671358	1338.009755	18.419815	-0.041577	2.099633
215.730386	1330.091248	18.424819	-0.041583	2.094312
215.311702	1322.175913	18.429824	-0.041500	2.088934
215.471676	1314.218588	18.434829	-0.041525	2.083570
215.490869	1306.311303	18.439834	-0.041524	2.078212
215.228431	1298.403710	18.444839	-0.041470	2.072812
215.258638	1290.441017	18.449843	-0.041470	2.067390
215.354338	1282.493933	18.454848	-0.041483	2.061970
215.180041	1274.598503	18.459853	-0.041446	2.056545
215.139498	1266.662201	18.464858	-0.041433	2.051090
215.207650	1258.711829	18.469863	-0.041441	2.045623
215.244845	1250.803439	18.474867	-0.041443	2.040166
214.822418	1242.935570	18.479872	-0.041359	2.034676
214.918987	1234.946332	18.484877	-0.041372	2.029140
214.995082	1227.005554	18.489882	-0.041381	2.023621
214.643807	1219.123554	18.494887	-0.041311	2.018083
214.851177	1211.158125	18.499891	-0.041345	2.012529
214.934346	1203.202006	18.504896	-0.041355	2.006954
214.824642	1195.310226	18.509901	-0.041330	2.001388
214.812280	1187.402598	18.514906	-0.041322	1.995806
214.367114	1179.523473	18.519911	-0.041235	1.990183
214.380708	1171.595163	18.524915	-0.041232	1.984557
214.229546	1163.676834	18.529920	-0.041199	1.978905
214.134832	1155.761007	18.534925	-0.041176	1.973245
214.211928	1147.803735	18.539930	-0.041186	1.967557
214.046708	1139.908449	18.544935	-0.041150	1.961871
214.061014	1132.005157	18.549939	-0.041148	1.956182
214.104288	1124.017945	18.554944	-0.041151	1.950418
213.982247	1116.098894	18.559949	-0.041123	1.944669
213.875649	1108.202938	18.564954	-0.041098	1.938922
213.799337	1100.280112	18.569959	-0.041079	1.933141
213.764383	1092.363905	18.574963	-0.041067	1.927352
213.684248	1084.455756	18.579968	-0.041048	1.921547
213.736703	1076.536453	18.584973	-0.041052	1.915731
213.800811	1068.607234	18.589978	-0.041059	1.909890
213.634926	1060.707313	18.594983	-0.041023	1.904028
213.602013	1052.814178	18.599987	-0.041012	1.898168
213.402406	1044.912097	18.604992	-0.040970	1.892264
213.306236	1037.000505	18.609997	-0.040947	1.886346
213.177069	1029.115482	18.615002	-0.040918	1.880426
213.000452	1021.227959	18.620007	-0.040880	1.874479
213.200976	1013.268316	18.625011	-0.040913	1.868503
212.941950	1005.377777	18.630016	-0.040860	1.862506
212.928872	997.476230	18.635021	-0.040852	1.856511
212.904721	989.565018	18.640026	-0.040843	1.850487
212.921334	981.638802	18.645031	-0.040841	1.844437
212.731855	973.784432	18.650035	-0.040801	1.838397
212.749327	965.863549	18.655040	-0.040799	1.832312
212.670084	957.966436	18.660045	-0.040779	1.826212
212.646721	950.065571	18.665050	-0.040770	1.820096
212.592817	942.174276	18.670055	-0.040755	1.813963
212.660874	934.258418	18.675059	-0.040762	1.807805
212.523670	926.382647	18.680064	-0.040732	1.801633
212.340929	918.526897	18.685069	-0.040693	1.795449
212.214636	910.584051	18.690074	-0.040664	1.789182
212.133609	902.683973	18.695079	-0.040644	1.782932
212.095717	894.809831	18.700083	-0.040632	1.776687
211.939020	886.912120	18.705088	-0.040598	1.770385
212.053623	879.005996	18.710093	-0.040615	1.764088
211.763492	871.173800	18.715098	-0.040556	1.757778
211.588004	863.289249	18.720103	-0.040518	1.751417
211.848701	855.357301	18.725107	-0.040562	1.745049
211.683077	847.498852	18.730112	-0.040526	1.738663
211.407908	839.654550	18.735117	-0.040470	1.732252
211.434228	831.746902	18.740122	-0.040470	1.725803
211.411440	823.869030	18.745127	-0.040460	1.719349
211.457401	815.993399	18.750131	-0.040464	1.712881
211.243450	808.110020	18.755136	-0.040419	1.706348
211.217543	800.228820	18.760141	-0.040409	1.699816
211.183464	792.373176	18.765146	-0.040398	1.693279
210.946484	784.497443	18.770151	-0.040349	1.686674
211.074210	776.618410	18.775155	-0.040368	1.680088
211.038985	768.760738	18.780160	-0.040356	1.673472
210.896038	760.886845	18.785165	-0.040325	1.666802
210.903816	753.022253	18.790170	-0.040321	1.660133
210.877653	745.158001	18.795175	-0.040311	1.653433
210.731100	737.311059	18.800179	-0.040279	1.646704
210.375438	729.496240	18.805184	-0.040208	1.639947
210.451893	721.609875	18.810189	-0.040217	1.633159
210.531392	713.688182	18.815194	-0.040227	1.626312
210.260509	705.858287	18.820199	-0.040172	1.619468
210.442230	697.986498	18.825203	-0.040201	1.612622
210.364109	690.120454	18.830208	-0.040181	1.605714
209.985472	682.338840	18.835213	-0.040106	1.598809
210.067183	674.470291	18.840218	-0.040116	1.591862
210.018046	666.609121	18.845223	-0.040102	1.584873
210.072137	658.768759	18.850227	-0.040107	1.577886
209.624306	650.969778	18.855232	-0.040019	1.570833
209.644222	643.117858	18.860237	-0.040017	1.563767
209.667891	635.286590	18.865242	-0.040017	1.556690
209.301081	627.471950	18.870247	-0.039944	1.549537
209.392061	619.604814	18.875251	-0.039956	1.542371
209.422866	611.759361	18.880256	-0.039957	1.535182
209.289401	603.938180	18.885261	-0.039927	1.527958
209.140548	596.130815	18.890266	-0.039894	1.520709
209.217114	588.291382	18.895271	-0.039903	1.513430
209.037648	580.480416	18.900275	-0.039865	1.506104
208.772239	572.695738	18.905280	-0.039811	1.498753
208.787257	564.858582	18.910285	-0.039809	1.491359
208.755323	557.041096	18.915290	-0.039798	1.483940
208.568632	549.255002	18.920295	-0.039758	1.476490
208.661178	541.378337	18.925299	-0.039770	1.468958
208.662226	533.557846	18.930304	-0.039766	1.461428
208.423760	525.792327	18.935309	-0.039716	1.453874
208.281558	517.997263	18.940314	-0.039685	1.446266
208.269097	510.192771	18.945319	-0.039678	1.438631
208.239404	502.405230	18.950323	-0.039667	1.430968
208.242425	494.589833	18.955328	-0.039663	1.423242
208.223326	486.810701	18.960333	-0.039655	1.415506
208.279476	479.010613	18.965338	-0.039660	1.407719
208.035286	471.267489	18.970343	-0.039610	1.399896
208.085855	463.482742	18.975347	-0.039614	1.392036
207.894989	455.710358	18.980352	-0.039574	1.384104
207.752835	447.954152	18.985357	-0.039542	1.376150
207.679209	440.184811	18.990362	-0.039524	1.368149
207.610493	432.423651	18.995367	-0.039506	1.360110
207.564541	424.677909	19.000371	-0.039493	1.352042
207.239609	416.945671	19.005376	-0.039427	1.343892
207.145359	409.208027	19.010381	-0.039405	1.335727
207.249880	401.424257	19.015386	-0.039420	1.327498
207.080293	393.698782	19.020391	-0.039383	1.319231
206.972406	385.893921	19.025395	-0.039358	1.310837
206.911833	378.107968	19.030400	-0.039342	1.302418
206.749850	370.406726	19.035405	-0.039307	1.294019
206.715571	362.679372	19.040410	-0.039296	1.285559
206.619129	354.980390	19.045415	-0.039273	1.277063
206.693279	347.251129	19.050419	-0.039282	1.268508
206.635164	339.541280	19.055424	-0.039266	1.259892
206.517470	331.854766	19.060429	-0.039239	1.251232
206.488557	324.162580	19.065434	-0.039229	1.242521
206.253214	316.500272	19.070439	-0.039181	1.233744
206.187306	308.801311	19.075443	-0.039163	1.224894
206.204486	301.106040	19.080448	-0.039162	1.216001
206.102289	293.434511	19.085453	-0.039138	1.207046
205.900230	285.806243	19.090458	-0.039096	1.198055
205.778687	278.145535	19.095463	-0.039068	1.188973
205.738909	270.492179	19.100467	-0.039056	1.179847
205.654938	262.845453	19.105472	-0.039035	1.170649
205.352668	255.240477	19.110477	-0.038974	1.161384
205.399727	247.582513	19.115482	-0.038978	1.152052
205.525890	239.888138	19.120487	-0.038997	1.142615
205.419355	232.288217	19.125491	-0.038972	1.133168
205.231270	224.690636	19.130496	-0.038933	1.123627
204.990976	217.129154	19.135501	-0.038883	1.114039
204.942663	209.523109	19.140506	-0.038869	1.104352
204.665312	201.972723	19.145511	-0.038813	1.094600
204.754403	194.368391	19.150515	-0.038825	1.084773
204.499556	186.836907	19.155520	-0.038773	1.074873
204.728666	179.213010	19.160525	-0.038810	1.064870
204.583962	171.691413	19.165530	-0.038779	1.054822
204.320348	164.175915	19.170535	-0.038725	1.044658
204.245236	156.666553	19.175539	-0.038706	1.034447
204.173201	149.146176	19.180544	-0.038688	1.024120
204.025697	141.660921	19.185549	-0.038656	1.013718
203.913502	134.181285	19.190554	-0.038630	1.003225
203.815485	126.700338	19.195559	-0.038607	0.992622
203.825404	119.197142	19.200563	-0.038604	0.981900
203.522726	111.783321	19.205568	-0.038543	0.971110
203.260002	104.376417	19.210573	-0.038490	0.960219
203.287125	96.939427	19.215578	-0.038490	0.949233
203.084186	89.551357	19.220583	-0.038448	0.938132
203.067373	82.148216	19.225587	-0.038440	0.926925
202.906706	74.800772	19.230592	-0.038406	0.915627
202.829555	67.428761	19.235597	-0.038387	0.904173
202.436245	60.377636	19.240602	-0.038309	0.892991