Thu Mar 11 18:24:02 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.314429	0.129298	0.000000	0.000027	0.724160

0.302209	0.178674	0.005005	0.000029	0.724252
0.306552	0.069953	0.010010	0.000028	0.724041
0.361632	0.011629	0.015014	0.000017	0.723947
0.445285	-0.004647	0.020019	0.000002	0.723944
0.745774	-0.054389	0.025024	-0.000055	0.723952
0.528055	-0.020277	0.030029	-0.000014	0.723943
0.435470	-0.001431	0.035034	0.000003	0.723948
0.614235	-0.032530	0.040038	-0.000031	0.723950
0.342945	0.014148	0.045043	0.000020	0.723947
0.334046	0.019330	0.050048	0.000021	0.723955
0.487585	-0.013333	0.055053	-0.000008	0.723945
0.533510	-0.019665	0.060058	-0.000016	0.723949
0.410856	0.002781	0.065062	0.000006	0.723950
0.431065	-0.002957	0.070067	0.000002	0.723946
0.455920	-0.020438	0.075072	-0.000003	0.723921
0.404302	-0.162358	0.080077	0.000007	0.723625
0.448796	-0.166604	0.085082	-0.000002	0.723633
0.502609	-0.178484	0.090086	-0.000012	0.723629
0.407588	-0.163466	0.095091	0.000006	0.723625
0.531239	-0.180572	0.100096	-0.000018	0.723635
0.382247	-0.158533	0.105101	0.000010	0.723627
0.419009	-0.257367	0.110106	0.000003	0.723446
0.525791	-0.333336	0.115110	-0.000017	0.723335
0.560287	-0.339706	0.120115	-0.000024	0.723335
0.530945	-0.331126	0.125120	-0.000018	0.723342
0.293443	-0.293327	0.130125	0.000026	0.723334
0.342161	-0.417373	0.135130	0.000016	0.723108
0.470499	-0.494807	0.140134	-0.000008	0.723001
0.439127	-0.489966	0.145139	-0.000002	0.723000
0.420248	-0.484445	0.150144	0.000001	0.723005
0.391294	-0.557058	0.155149	0.000007	0.722852
0.314346	-0.625922	0.160154	0.000021	0.722691
0.528241	-0.664871	0.165158	-0.000019	0.722689
0.449413	-0.653608	0.170163	-0.000005	0.722684
0.450742	-0.770227	0.175168	-0.000005	0.722456
0.199137	-0.772050	0.180173	0.000042	0.722365
0.302164	-0.789629	0.185178	0.000022	0.722367
0.308660	-0.839748	0.190182	0.000021	0.722271
0.255250	-0.934672	0.195187	0.000031	0.722066
0.175054	-0.915057	0.200192	0.000045	0.722077
0.178313	-0.939508	0.205197	0.000045	0.722031
0.232937	-1.096573	0.210202	0.000034	0.721742
0.277830	-1.104755	0.215206	0.000026	0.721742
0.345547	-1.147980	0.220211	0.000013	0.721681
0.164732	-1.240302	0.225216	0.000046	0.721436
-0.002773	-1.214354	0.230221	0.000077	0.721429
-0.160277	-1.235762	0.235226	0.000107	0.721332
0.237285	-1.416133	0.240230	0.000033	0.721117
0.181814	-1.409737	0.245235	0.000043	0.721111
0.125383	-1.479832	0.250240	0.000053	0.720953
0.133434	-1.525015	0.255245	0.000051	0.720868
0.192061	-1.566585	0.260250	0.000040	0.720807
-0.102968	-1.649954	0.265254	0.000095	0.720540
-0.364274	-1.607454	0.270259	0.000143	0.720532
0.004509	-1.778539	0.275264	0.000075	0.720325
-0.550280	-1.735263	0.280269	0.000178	0.720216
-0.665321	-1.748057	0.285274	0.000199	0.720151
-0.670393	-1.876318	0.290278	0.000200	0.719897
-1.236258	-1.777792	0.295283	0.000305	0.719893
-1.663882	-1.793406	0.300288	0.000384	0.719712
-2.558072	-1.693671	0.305293	0.000551	0.719595
-2.745364	-1.658049	0.310298	0.000585	0.719600
-2.482895	-1.782547	0.315302	0.000536	0.719447
-3.410836	-1.712557	0.320307	0.000709	0.719260
-3.356171	-1.717889	0.325312	0.000698	0.719269
-3.768772	-1.648275	0.330317	0.000775	0.719262
-4.082956	-1.740740	0.335322	0.000833	0.718969
-4.561944	-1.660170	0.340326	0.000922	0.718960
-4.902757	-1.603378	0.345331	0.000986	0.718953
-4.580202	-1.657887	0.350336	0.000925	0.718959
-4.999579	-1.710987	0.355341	0.001003	0.718707
-5.975982	-1.571164	0.360346	0.001185	0.718641
-5.415984	-1.671644	0.365350	0.001080	0.718639
-5.379965	-1.680936	0.370355	0.001074	0.718634
-5.705763	-1.627763	0.375360	0.001134	0.718625
-6.270838	-1.669909	0.380365	0.001239	0.718343
-6.002099	-1.714720	0.385370	0.001189	0.718350
-6.672157	-1.595130	0.390374	0.001313	0.718351
-6.834950	-1.569841	0.395379	0.001343	0.718344
-6.206555	-1.676931	0.400384	0.001226	0.718354
-7.096376	-1.676429	0.405389	0.001392	0.718042
-7.614879	-1.599041	0.410394	0.001488	0.718013
-7.426817	-1.631895	0.415398	0.001453	0.718014
-7.509622	-1.620890	0.420403	0.001468	0.718007
-7.638491	-1.592949	0.425408	0.001492	0.718018
-7.504189	-1.620100	0.430413	0.001467	0.718012
-7.767811	-1.727219	0.435418	0.001516	0.717708
-8.568109	-1.588297	0.440422	0.001664	0.717701
-9.047950	-1.505229	0.445427	0.001753	0.717696
-8.246671	-1.643477	0.450432	0.001604	0.717706
-8.383325	-1.624616	0.455437	0.001629	0.717695
-8.730627	-1.562668	0.460442	0.001694	0.717696
-8.447432	-1.698504	0.465446	0.001641	0.717527
-9.600951	-1.572414	0.470451	0.001855	0.717371
-9.064729	-1.664088	0.475456	0.001755	0.717379
-9.338719	-1.619893	0.480461	0.001806	0.717370
-9.607524	-1.569083	0.485466	0.001856	0.717376
-8.977437	-1.680713	0.490470	0.001739	0.717378
-9.667019	-1.566558	0.495475	0.001867	0.717361
-10.066986	-1.634644	0.500480	0.001941	0.717086
-10.079647	-1.638218	0.505485	0.001943	0.717074
-10.793779	-1.507612	0.510490	0.002076	0.717082
-10.150016	-1.619392	0.515494	0.001956	0.717088
-10.089839	-1.636729	0.520499	0.001945	0.717075
-10.262174	-1.601604	0.525504	0.001976	0.717084
-10.500281	-1.584629	0.530509	0.002021	0.717034
-11.044390	-1.629771	0.535514	0.002122	0.716753
-10.626059	-1.703252	0.540518	0.002044	0.716756
-11.452704	-1.558439	0.545523	0.002197	0.716751
-11.030373	-1.630701	0.550528	0.002119	0.716758
-10.976884	-1.643256	0.555533	0.002108	0.716752
-11.360803	-1.574150	0.560538	0.002180	0.716754
-11.207743	-1.667649	0.565542	0.002151	0.716623
-12.211029	-1.581091	0.570547	0.002338	0.716441
-11.886095	-1.636244	0.575552	0.002277	0.716447
-12.243381	-1.576374	0.580557	0.002343	0.716440
-12.166143	-1.588902	0.585562	0.002329	0.716442
-11.714517	-1.667173	0.590566	0.002244	0.716447
-12.362447	-1.556083	0.595571	0.002365	0.716439
-12.228304	-1.620959	0.600576	0.002340	0.716358
-13.019481	-1.597362	0.605581	0.002487	0.716126
-12.945801	-1.610399	0.610586	0.002473	0.716127
-13.308368	-1.542494	0.615590	0.002540	0.716134
-12.965195	-1.609171	0.620595	0.002476	0.716123
-12.550913	-1.679494	0.625600	0.002399	0.716130
-13.059763	-1.592662	0.630605	0.002493	0.716123
-13.083537	-1.605949	0.635610	0.002497	0.716089
-13.169249	-1.696316	0.640614	0.002513	0.715880
-13.799787	-1.585992	0.645619	0.002630	0.715876
-13.742276	-1.592998	0.650624	0.002620	0.715883
-13.241498	-1.687435	0.655629	0.002526	0.715873
-13.501248	-1.640682	0.660634	0.002574	0.715874
-13.725500	-1.599189	0.665638	0.002616	0.715878
-13.975052	-1.700257	0.670643	0.002662	0.715590
-14.680894	-1.599269	0.675648	0.002793	0.715541
-15.086252	-1.529449	0.680653	0.002869	0.715537
-14.675097	-1.602015	0.685658	0.002792	0.715538
-14.567512	-1.619322	0.690662	0.002772	0.715542
-14.953939	-1.555039	0.695667	0.002843	0.715534
-14.747976	-1.588100	0.700672	0.002805	0.715541
-14.844470	-1.655839	0.705677	0.002823	0.715373
-15.817963	-1.557841	0.710682	0.003004	0.715224
-15.354133	-1.637668	0.715686	0.002917	0.715230
-15.542850	-1.606637	0.720691	0.002952	0.715225
-15.353593	-1.635740	0.725696	0.002917	0.715235
-15.775145	-1.565000	0.730701	0.002995	0.715226
-15.972089	-1.530851	0.735706	0.003031	0.715225
-15.557302	-1.663277	0.740710	0.002954	0.715109
-16.749128	-1.556948	0.745715	0.003176	0.714899
-16.541863	-1.588909	0.750720	0.003137	0.714909
-16.507962	-1.599305	0.755725	0.003130	0.714901
-16.324954	-1.630916	0.760730	0.003096	0.714903
-16.353809	-1.623053	0.765734	0.003101	0.714909
-16.766653	-1.555355	0.770739	0.003178	0.714898
-16.295923	-1.677314	0.775744	0.003090	0.714823
-17.279854	-1.613477	0.780749	0.003273	0.714602
-17.257867	-1.617228	0.785754	0.003269	0.714603
-17.250456	-1.617321	0.790758	0.003267	0.714605
-17.362263	-1.599595	0.795763	0.003288	0.714601
-17.535302	-1.565220	0.800768	0.003320	0.714609
-17.393638	-1.593320	0.805773	0.003293	0.714604
-17.280344	-1.659446	0.810778	0.003272	0.714513
-18.287535	-1.598758	0.815782	0.003459	0.714277
-18.363803	-1.588894	0.820787	0.003473	0.714270
-18.207327	-1.610280	0.825792	0.003444	0.714283
-18.070364	-1.639584	0.830797	0.003418	0.714274
-18.532843	-1.558123	0.835802	0.003504	0.714273
-18.359736	-1.585773	0.840806	0.003472	0.714279
-18.224667	-1.615525	0.845811	0.003447	0.714268
-18.789334	-1.664896	0.850816	0.003551	0.713971
-19.142194	-1.605516	0.855821	0.003617	0.713964
-19.274062	-1.582485	0.860826	0.003641	0.713964
-19.186145	-1.596058	0.865830	0.003625	0.713968
-19.405974	-1.563600	0.870835	0.003665	0.713955
-19.095357	-1.613866	0.875840	0.003607	0.713966
-18.933354	-1.644566	0.880845	0.003577	0.713962
-20.037344	-1.593382	0.885850	0.003782	0.713674
-19.827195	-1.642435	0.890854	0.003743	0.713651
-20.174162	-1.584573	0.895859	0.003808	0.713643
-20.217530	-1.572402	0.900864	0.003815	0.713653
-20.381250	-1.546914	0.905869	0.003846	0.713646
-20.083600	-1.599505	0.910874	0.003790	0.713647
-19.906006	-1.629175	0.915878	0.003757	0.713651
-20.490703	-1.601218	0.920883	0.003865	0.713500
-21.048490	-1.572662	0.925888	0.003969	0.713359
-20.572658	-1.659905	0.930893	0.003880	0.713355
-21.173851	-1.554115	0.935898	0.003992	0.713353
-21.138111	-1.560239	0.940902	0.003985	0.713354
-20.911984	-1.603934	0.945907	0.003943	0.713347
-21.090136	-1.568457	0.950912	0.003976	0.713355
-21.106597	-1.615423	0.955917	0.003979	0.713256
-21.832124	-1.606097	0.960922	0.004114	0.713018
-21.419158	-1.677590	0.965926	0.004037	0.713022
-22.212529	-1.541753	0.970931	0.004184	0.713012
-21.869845	-1.597783	0.975936	0.004120	0.713022
-21.715246	-1.628497	0.980941	0.004091	0.713016
-22.179292	-1.547415	0.985946	0.004177	0.713013
-21.737600	-1.662655	0.990950	0.004095	0.712941
-22.580358	-1.633638	0.995955	0.004252	0.712700
-22.485436	-1.646388	1.000960	0.004234	0.712709
-22.861494	-1.582471	1.005965	0.004304	0.712703
-22.852586	-1.584560	1.010970	0.004302	0.712702
-22.568341	-1.633944	1.015974	0.004249	0.712705
-23.234153	-1.520241	1.020979	0.004372	0.712696
-23.001134	-1.573904	1.025984	0.004329	0.712672
-23.612554	-1.611368	1.030989	0.004442	0.712381
-23.772719	-1.582860	1.035994	0.004472	0.712381
-23.961602	-1.545435	1.040998	0.004507	0.712389
-23.739254	-1.590962	1.046003	0.004465	0.712378
-23.719143	-1.591951	1.051008	0.004462	0.712383
-24.324138	-1.487200	1.056013	0.004574	0.712378
-23.918322	-1.560207	1.061018	0.004498	0.712377
-23.509783	-1.689724	1.066022	0.004422	0.712264
-25.026568	-1.513063	1.071027	0.004704	0.712078
-24.543112	-1.593052	1.076032	0.004614	0.712090
-24.408503	-1.620594	1.081037	0.004589	0.712084
-24.839241	-1.545165	1.086042	0.004669	0.712081
-24.568257	-1.591407	1.091046	0.004618	0.712086
-24.696030	-1.572665	1.096051	0.004642	0.712078
-24.565077	-1.638287	1.101056	0.004617	0.711994
-25.647929	-1.567052	1.106061	0.004818	0.711752
-25.396873	-1.611193	1.111066	0.004772	0.711754
-25.423776	-1.603612	1.116070	0.004776	0.711760
-25.913119	-1.521927	1.121075	0.004867	0.711749
-25.632183	-1.567008	1.126080	0.004815	0.711759
-25.587299	-1.578326	1.131085	0.004806	0.711753
-25.808245	-1.539025	1.136090	0.004847	0.711753
-26.026696	-1.622596	1.141094	0.004888	0.711509
-26.598423	-1.554752	1.146099	0.004994	0.711442
-26.229338	-1.617266	1.151104	0.004925	0.711449
-26.387904	-1.590059	1.156109	0.004954	0.711447
-26.720527	-1.530310	1.161114	0.005016	0.711448
-26.259028	-1.610348	1.166118	0.004930	0.711453
-26.599799	-1.554273	1.171123	0.004993	0.711444
-26.867159	-1.612369	1.176128	0.005043	0.711234
-27.456963	-1.557872	1.181133	0.005152	0.711133
-27.445934	-1.561315	1.186138	0.005150	0.711130
-27.469903	-1.555550	1.191142	0.005154	0.711134
-27.647072	-1.526435	1.196147	0.005187	0.711129
-27.350085	-1.576808	1.201152	0.005132	0.711135
-27.651084	-1.523358	1.206157	0.005188	0.711135
-27.560494	-1.563389	1.211162	0.005170	0.711087
-27.591069	-1.666674	1.216166	0.005176	0.710871
-28.082724	-1.585112	1.221171	0.005267	0.710859
-28.364578	-1.532884	1.226176	0.005320	0.710863
-28.158463	-1.570271	1.231181	0.005281	0.710862
-28.203803	-1.562301	1.236186	0.005289	0.710863
-28.304945	-1.540751	1.241190	0.005308	0.710870
-28.410938	-1.588974	1.246195	0.005327	0.710736
-29.153876	-1.560332	1.251200	0.005466	0.710530
-29.004048	-1.589096	1.256205	0.005438	0.710526
-29.283814	-1.538295	1.261210	0.005489	0.710528
-28.836721	-1.615500	1.266214	0.005406	0.710533
-29.179618	-1.558411	1.271219	0.005470	0.710526
-29.293447	-1.534016	1.276224	0.005491	0.710534
-29.075611	-1.614441	1.281229	0.005450	0.710452
-29.932322	-1.581608	1.286234	0.005609	0.710213
-29.891436	-1.585489	1.291238	0.005601	0.710220
-30.420240	-1.496438	1.296243	0.005700	0.710210
-29.891997	-1.587757	1.301248	0.005601	0.710216
-29.926423	-1.583567	1.306253	0.005607	0.710212
-30.290812	-1.519052	1.311258	0.005675	0.710212
-29.768193	-1.643034	1.316262	0.005577	0.710150
-30.821607	-1.588989	1.321267	0.005773	0.709884
-30.955742	-1.560158	1.326272	0.005798	0.709894
-30.864096	-1.580777	1.331277	0.005781	0.709886
-30.688432	-1.612856	1.336282	0.005748	0.709884
-30.724148	-1.603166	1.341286	0.005754	0.709891
-31.228798	-1.517673	1.346291	0.005848	0.709883
-30.711865	-1.645743	1.351296	0.005752	0.709811
-31.656797	-1.589538	1.356301	0.005928	0.709587
-31.817336	-1.560646	1.361306	0.005957	0.709588
-31.641320	-1.589355	1.366310	0.005924	0.709594
-31.694466	-1.584793	1.371315	0.005934	0.709585
-31.649539	-1.587642	1.376320	0.005925	0.709595
-31.693804	-1.581072	1.381325	0.005933	0.709593
-31.847011	-1.621456	1.386330	0.005962	0.709458
-32.841899	-1.542829	1.391334	0.006147	0.709261
-32.854391	-1.544262	1.396339	0.006149	0.709254
-32.403823	-1.620695	1.401344	0.006065	0.709262
-32.650878	-1.577983	1.406349	0.006111	0.709260
-32.913775	-1.532058	1.411354	0.006159	0.709258
-32.645708	-1.576784	1.416358	0.006109	0.709265
-32.628045	-1.599738	1.421363	0.006106	0.709226
-33.494636	-1.582029	1.426368	0.006267	0.708952
-33.695318	-1.546489	1.431373	0.006304	0.708952
-33.763115	-1.537479	1.436378	0.006317	0.708946
-33.406063	-1.597560	1.441382	0.006250	0.708954
-33.745063	-1.541423	1.446387	0.006313	0.708946
-33.404471	-1.599467	1.451392	0.006249	0.708951
-33.518894	-1.579418	1.456397	0.006270	0.708951
-34.281755	-1.587153	1.461402	0.006412	0.708664
-34.408252	-1.578278	1.466406	0.006436	0.708637
-34.510580	-1.564085	1.471411	0.006454	0.708629
-34.539031	-1.553825	1.476416	0.006459	0.708640
-34.688792	-1.529776	1.481421	0.006487	0.708635
-34.356800	-1.590576	1.486426	0.006425	0.708632
-34.226244	-1.610293	1.491430	0.006401	0.708639
-34.992463	-1.581213	1.496435	0.006543	0.708425
-35.529128	-1.524351	1.501440	0.006643	0.708347
-35.140403	-1.594796	1.506445	0.006570	0.708345
-35.417709	-1.545987	1.511450	0.006622	0.708344
-35.269997	-1.570165	1.516454	0.006594	0.708349
-35.202582	-1.586069	1.521459	0.006581	0.708342
-35.163505	-1.590262	1.526464	0.006574	0.708348
-35.545332	-1.645687	1.531469	0.006645	0.708100
-36.653237	-1.495825	1.536474	0.006851	0.708005
-36.107219	-1.589752	1.541478	0.006749	0.708013
-36.422259	-1.538616	1.546483	0.006807	0.708003
-36.261203	-1.562683	1.551488	0.006777	0.708013
-36.033099	-1.605006	1.556493	0.006735	0.708010
-36.509737	-1.522069	1.561498	0.006823	0.708006
-36.534759	-1.588798	1.566502	0.006828	0.707864
-37.188923	-1.558276	1.571507	0.006949	0.707691
-36.945937	-1.599284	1.576512	0.006904	0.707696
-37.180967	-1.557696	1.581517	0.006947	0.707696
-37.237769	-1.549978	1.586522	0.006958	0.707692
-36.689649	-1.642027	1.591526	0.006855	0.707703
-37.375528	-1.526694	1.596531	0.006983	0.707690
-37.426207	-1.581619	1.601536	0.006992	0.707562
-38.031291	-1.569023	1.606541	0.007105	0.707371
-38.134570	-1.552630	1.611546	0.007124	0.707368
-37.998704	-1.571590	1.616550	0.007098	0.707378
-37.890811	-1.595365	1.621555	0.007078	0.707370
-37.882307	-1.594269	1.626560	0.007076	0.707375
-38.175554	-1.543781	1.631565	0.007130	0.707372
-38.374011	-1.539591	1.636570	0.007167	0.707310
-38.771706	-1.582196	1.641574	0.007241	0.707082
-39.093497	-1.527941	1.646579	0.007301	0.707077
-39.309323	-1.487326	1.651584	0.007341	0.707081
-38.705336	-1.594280	1.656589	0.007228	0.707083
-39.140471	-1.518383	1.661594	0.007309	0.707080
-38.977764	-1.545862	1.666598	0.007278	0.707084
-38.877188	-1.567710	1.671603	0.007260	0.707076
-39.485933	-1.609379	1.676608	0.007373	0.706775
-39.961137	-1.536790	1.681613	0.007461	0.706751
-40.026949	-1.526801	1.686618	0.007473	0.706748
-39.293360	-1.654023	1.691622	0.007336	0.706755
-40.072775	-1.521495	1.696627	0.007481	0.706743
-40.034273	-1.525243	1.701632	0.007474	0.706749
-39.576972	-1.607257	1.706637	0.007389	0.706749
-40.597153	-1.561994	1.711642	0.007578	0.706475
-40.802201	-1.540196	1.716646	0.007616	0.706446
-40.684043	-1.566417	1.721651	0.007594	0.706436
-40.401064	-1.614330	1.726656	0.007541	0.706441
-40.752137	-1.552791	1.731661	0.007606	0.706439
-40.808227	-1.542670	1.736666	0.007617	0.706440
-40.285050	-1.633127	1.741670	0.007519	0.706446
-41.347762	-1.595902	1.746675	0.007717	0.706140
-41.670749	-1.543988	1.751680	0.007777	0.706129
-41.342514	-1.602804	1.756685	0.007715	0.706129
-41.741370	-1.535463	1.761690	0.007789	0.706122
-41.828642	-1.515241	1.766694	0.007805	0.706132
-41.757817	-1.533256	1.771699	0.007792	0.706121
-41.489786	-1.576914	1.776704	0.007742	0.706130
-41.662755	-1.645871	1.781709	0.007774	0.705930
-42.622223	-1.513790	1.786714	0.007952	0.705852
-41.903802	-1.637234	1.791718	0.007818	0.705861
-42.248309	-1.581558	1.796723	0.007882	0.705850
-42.816646	-1.474766	1.801728	0.007988	0.705862
-42.246729	-1.577210	1.806733	0.007882	0.705860
-42.392018	-1.563954	1.811738	0.007909	0.705835
-43.200397	-1.573357	1.816742	0.008059	0.705527
-43.327176	-1.553969	1.821747	0.008082	0.705521
-43.132594	-1.586867	1.826752	0.008046	0.705525
-43.138169	-1.585402	1.831757	0.008047	0.705526
-43.604799	-1.505469	1.836762	0.008133	0.705520
-43.271011	-1.562717	1.841766	0.008071	0.705525
-43.484739	-1.527635	1.846771	0.008111	0.705519
-43.869994	-1.605376	1.851776	0.008182	0.705225
-43.925314	-1.601129	1.856781	0.008192	0.705214
-44.383200	-1.521046	1.861786	0.008277	0.705211
-44.223141	-1.546279	1.866790	0.008247	0.705218
-44.308957	-1.534115	1.871795	0.008263	0.705212
-44.276455	-1.539438	1.876800	0.008257	0.705213
-44.130173	-1.564928	1.881805	0.008229	0.705215
-44.959860	-1.570617	1.886810	0.008384	0.704906
-44.774536	-1.610044	1.891814	0.008349	0.704894
-45.108037	-1.555698	1.896819	0.008411	0.704884
-45.106532	-1.551504	1.901824	0.008410	0.704893
-45.037078	-1.565431	1.906829	0.008397	0.704890
-45.233113	-1.534584	1.911834	0.008434	0.704882
-45.093351	-1.553294	1.916838	0.008407	0.704895
-45.684134	-1.582868	1.921843	0.008517	0.704624
-46.062093	-1.532755	1.926848	0.008587	0.704589
-45.942369	-1.553551	1.931853	0.008565	0.704591
-46.109945	-1.527621	1.936858	0.008596	0.704583
-45.879618	-1.564301	1.941862	0.008553	0.704593
-46.013663	-1.543264	1.946867	0.008578	0.704587
-45.940592	-1.554814	1.951872	0.008564	0.704591
-46.076092	-1.655116	1.956877	0.008589	0.704340
-47.017158	-1.528954	1.961882	0.008764	0.704257
-46.869847	-1.551611	1.966886	0.008736	0.704264
-46.988173	-1.536162	1.971891	0.008758	0.704253
-46.788294	-1.569469	1.976896	0.008721	0.704258
-46.686333	-1.587293	1.981901	0.008701	0.704259
-46.936703	-1.543541	1.986906	0.008748	0.704258
-46.994463	-1.654159	1.991910	0.008759	0.704015
-48.018184	-1.505846	1.996915	0.008949	0.703946
-47.907368	-1.522801	2.001920	0.008928	0.703952

-47.583252	-1.579451	2.011917	0.008867	0.703955
-47.879060	-1.529878	2.021914	0.008922	0.703949
-47.679237	-1.566267	2.031910	0.008884	0.703949
-47.552912	-1.599819	2.041907	0.008861	0.703927
-48.249720	-1.550033	2.051904	0.008990	0.703778
-47.968557	-1.568113	2.061901	0.008937	0.703843
-47.937010	-1.523089	2.071898	0.008931	0.703946
-47.852371	-1.538942	2.081894	0.008915	0.703945
-47.460910	-1.606553	2.091891	0.008841	0.703950
-47.692535	-1.566098	2.101888	0.008884	0.703949
-47.692262	-1.565475	2.111885	0.008884	0.703952
-47.995194	-1.513314	2.121882	0.008940	0.703949
-47.816082	-1.545584	2.131878	0.008906	0.703949
-47.756170	-1.530565	2.141875	0.008894	0.704001
-46.993121	-1.539125	2.151872	0.008752	0.704259
-46.788043	-1.575791	2.161869	0.008713	0.704260
-46.890956	-1.558710	2.171866	0.008732	0.704258
-47.038955	-1.532932	2.181862	0.008759	0.704257
-46.526074	-1.523248	2.191859	0.008663	0.704462
-46.041641	-1.545809	2.201856	0.008573	0.704591
-46.005853	-1.551091	2.211853	0.008566	0.704594
-46.237228	-1.512738	2.221850	0.008608	0.704589
-45.421391	-1.565391	2.231846	0.008456	0.704777
-45.245973	-1.542569	2.241843	0.008423	0.704887
-45.329524	-1.527235	2.251840	0.008438	0.704888
-45.115056	-1.567591	2.261837	0.008398	0.704885
-44.901333	-1.469971	2.271834	0.008358	0.705159
-44.476813	-1.521455	2.281830	0.008278	0.705208
-44.441608	-1.527098	2.291827	0.008271	0.705210
-44.080199	-1.531767	2.301824	0.008204	0.705331
-43.306881	-1.573856	2.311821	0.008059	0.705525
-43.473954	-1.546079	2.321818	0.008090	0.705522
-43.269296	-1.583793	2.331814	0.008052	0.705520
-43.112492	-1.517542	2.341811	0.008022	0.705710
-42.614697	-1.532528	2.351808	0.007929	0.705859
-42.602171	-1.536496	2.361805	0.007926	0.705857
-42.532259	-1.547236	2.371802	0.007913	0.705861
-41.934858	-1.523758	2.381798	0.007801	0.706123
-41.769238	-1.550859	2.391795	0.007770	0.706129
-41.614026	-1.579563	2.401792	0.007741	0.706127
-41.439047	-1.515727	2.411789	0.007708	0.706319
-40.935900	-1.545753	2.421786	0.007613	0.706440
-40.769914	-1.576300	2.431782	0.007582	0.706438
-40.944653	-1.528065	2.441779	0.007614	0.706474
-40.095510	-1.542529	2.451776	0.007456	0.706749
-39.916469	-1.575131	2.461773	0.007422	0.706749
-39.988324	-1.562308	2.471770	0.007435	0.706750
-39.601405	-1.534216	2.481766	0.007363	0.706945
-39.246021	-1.530019	2.491763	0.007296	0.707082
-39.236248	-1.533499	2.501760	0.007294	0.707079
-39.359140	-1.475026	2.511757	0.007316	0.707153
-38.332374	-1.548501	2.521754	0.007125	0.707374
-38.254025	-1.563037	2.531750	0.007110	0.707373
-38.524172	-1.514169	2.541747	0.007160	0.707375
-37.561730	-1.545519	2.551744	0.006980	0.707657
-37.548198	-1.527735	2.561741	0.006977	0.707699
-37.405844	-1.553406	2.571738	0.006950	0.707699
-37.382438	-1.499350	2.581734	0.006946	0.707816
-36.494083	-1.560473	2.591731	0.006780	0.708012
-36.487783	-1.561737	2.601728	0.006778	0.708013
-36.783541	-1.511463	2.611725	0.006833	0.708008
-35.830015	-1.523809	2.621722	0.006655	0.708325
-35.658867	-1.544315	2.631718	0.006623	0.708346
-35.522620	-1.566595	2.641715	0.006597	0.708351
-35.444398	-1.533329	2.651712	0.006582	0.708446
-34.861898	-1.541598	2.661709	0.006473	0.708638
-34.876437	-1.540045	2.671706	0.006475	0.708637
-34.974564	-1.523087	2.681702	0.006493	0.708637
-34.100329	-1.529656	2.691699	0.006330	0.708936
-33.912240	-1.554146	2.701696	0.006295	0.708955
-33.939461	-1.548890	2.711693	0.006299	0.708957
-33.782421	-1.510772	2.721690	0.006270	0.709090
-32.996581	-1.566743	2.731686	0.006123	0.709259
-33.284664	-1.514917	2.741683	0.006176	0.709260
-32.953976	-1.572080	2.751680	0.006114	0.709265
-32.426453	-1.507686	2.761677	0.006016	0.709582
-31.972964	-1.584232	2.771674	0.005931	0.709592
-32.284876	-1.529761	2.781670	0.005989	0.709590
-31.991331	-1.523567	2.791667	0.005933	0.709708
-31.159811	-1.580403	2.801664	0.005778	0.709891
-31.505748	-1.520652	2.811661	0.005842	0.709888
-31.403026	-1.538904	2.821658	0.005823	0.709889
-30.940673	-1.459344	2.831654	0.005736	0.710214
-30.388452	-1.556176	2.841651	0.005633	0.710218
-30.360058	-1.562511	2.851648	0.005627	0.710216
-30.163863	-1.504684	2.861645	0.005590	0.710402
-29.539157	-1.551797	2.871642	0.005474	0.710531
-29.821499	-1.502874	2.881638	0.005526	0.710529
-29.424942	-1.551656	2.891635	0.005452	0.710573
-28.606838	-1.550042	2.901632	0.005299	0.710868
-28.494706	-1.571926	2.911629	0.005278	0.710865
-28.631830	-1.548883	2.921626	0.005303	0.710863
-28.619480	-1.491407	2.931622	0.005300	0.710983
-27.588454	-1.598726	2.941619	0.005108	0.711137
-27.916705	-1.541429	2.951616	0.005169	0.711135
-27.838491	-1.555742	2.961613	0.005154	0.711135
-27.227849	-1.510802	2.971610	0.005039	0.711442
-27.227938	-1.507166	2.981606	0.005039	0.711450
-27.101786	-1.528806	2.991603	0.005015	0.711453
-26.706817	-1.485652	3.001600	0.004941	0.711680
-26.305975	-1.518339	3.011597	0.004866	0.711758
-26.285117	-1.522548	3.021594	0.004862	0.711758
-26.032838	-1.498611	3.031590	0.004815	0.711896
-25.160332	-1.558119	3.041587	0.004652	0.712088
-25.394683	-1.516383	3.051584	0.004695	0.712089
-25.317493	-1.531296	3.061581	0.004680	0.712087
-24.802488	-1.476821	3.071578	0.004584	0.712379
-24.571795	-1.517557	3.081574	0.004541	0.712381
-24.523151	-1.525462	3.091571	0.004531	0.712383
-24.107654	-1.490514	3.101568	0.004453	0.712601
-23.567448	-1.534473	3.111565	0.004352	0.712706
-23.587910	-1.531791	3.121562	0.004356	0.712704
-23.627378	-1.497343	3.131558	0.004363	0.712760
-22.422190	-1.581558	3.141555	0.004138	0.713020
-22.649421	-1.542977	3.151552	0.004180	0.713017
-22.484337	-1.571549	3.161549	0.004149	0.713020
-22.286296	-1.526817	3.171546	0.004112	0.713180
-21.429612	-1.591953	3.181542	0.003952	0.713354
-21.751827	-1.534958	3.191539	0.004011	0.713354
-21.536125	-1.571329	3.201536	0.003971	0.713359
-21.012919	-1.574352	3.211533	0.003873	0.713539
-20.973070	-1.527590	3.221530	0.003865	0.713647
-20.789429	-1.561824	3.231526	0.003830	0.713645
-20.697928	-1.568793	3.241523	0.003813	0.713664
-20.138262	-1.516221	3.251520	0.003708	0.713968
-19.916382	-1.556481	3.261517	0.003667	0.713967
-20.114547	-1.523242	3.271514	0.003703	0.713964
-19.351508	-1.560727	3.281510	0.003561	0.714160
-18.989777	-1.568036	3.291507	0.003493	0.714274
-19.025056	-1.559962	3.301504	0.003499	0.714279
-18.885169	-1.586086	3.311501	0.003473	0.714277
-18.370697	-1.523550	3.321498	0.003377	0.714584
-18.044385	-1.571511	3.331494	0.003315	0.714605
-18.122724	-1.556119	3.341491	0.003330	0.714608
-18.097524	-1.500284	3.351488	0.003324	0.714729
-17.078735	-1.592626	3.361485	0.003134	0.714907
-17.358598	-1.544836	3.371482	0.003186	0.714903
-17.355797	-1.545277	3.381478	0.003185	0.714904
-16.779909	-1.491685	3.391475	0.003078	0.715215
-16.267942	-1.575426	3.401472	0.002982	0.715230
-16.246486	-1.579387	3.411469	0.002978	0.715231
-16.291986	-1.497346	3.421466	0.002986	0.715378
-15.261649	-1.599534	3.431462	0.002793	0.715540
-15.544888	-1.549255	3.441459	0.002846	0.715541
-15.352323	-1.582634	3.451456	0.002809	0.715543
-14.634652	-1.572325	3.461453	0.002675	0.715818
-14.414569	-1.583159	3.471450	0.002634	0.715875
-14.297444	-1.602940	3.481446	0.002612	0.715878
-14.337119	-1.595971	3.491443	0.002619	0.715878
-13.760524	-1.584800	3.501440	0.002511	0.716105
-13.712851	-1.581754	3.511437	0.002502	0.716128
-13.556071	-1.610333	3.521434	0.002472	0.716128
-13.457080	-1.569796	3.531430	0.002453	0.716244
-12.734212	-1.597680	3.541427	0.002318	0.716444
-12.468242	-1.643539	3.551424	0.002269	0.716448
-12.687685	-1.605258	3.561421	0.002309	0.716447
-12.228701	-1.572011	3.571418	0.002223	0.716676
-11.872336	-1.596698	3.581414	0.002156	0.716753
-11.814410	-1.606918	3.591411	0.002145	0.716754
-11.795430	-1.562657	3.601408	0.002141	0.716849
-10.935115	-1.597350	3.611405	0.001981	0.717084
-10.819964	-1.618868	3.621402	0.001959	0.717083
-10.864134	-1.612640	3.631398	0.001967	0.717081
-10.442010	-1.590024	3.641395	0.001888	0.717275
-9.857173	-1.640312	3.651392	0.001778	0.717382
-10.170884	-1.584651	3.661389	0.001836	0.717382
-9.968766	-1.611977	3.671386	0.001798	0.717400
-9.304289	-1.579463	3.681382	0.001674	0.717699
-8.914005	-1.648840	3.691379	0.001601	0.717700
-8.924181	-1.646809	3.701376	0.001603	0.717702
-8.883225	-1.582391	3.711373	0.001595	0.717844
-7.955839	-1.661443	3.721370	0.001422	0.718015
-8.067364	-1.642469	3.731366	0.001442	0.718014
-8.149482	-1.627347	3.741363	0.001457	0.718016
-7.507343	-1.630127	3.751360	0.001337	0.718237
-7.435372	-1.583366	3.761357	0.001323	0.718355
-7.360686	-1.598627	3.771354	0.001309	0.718352
-7.425417	-1.558778	3.781350	0.001321	0.718409
-6.382787	-1.626486	3.791347	0.001126	0.718642
-6.295864	-1.640719	3.801344	0.001109	0.718646
-6.536831	-1.598652	3.811341	0.001154	0.718645
-5.798177	-1.619424	3.821338	0.001016	0.718864
-5.599987	-1.605981	3.831334	0.000979	0.718961
-5.314560	-1.656755	3.841331	0.000925	0.718962
-5.427134	-1.637239	3.851328	0.000946	0.718961
-4.892794	-1.577147	3.861325	0.000846	0.719268
-4.675902	-1.616268	3.871322	0.000805	0.719268
-4.593991	-1.631628	3.881318	0.000789	0.719267
-4.338182	-1.592623	3.891315	0.000741	0.719435
-3.851796	-1.595891	3.901312	0.000650	0.719600
-3.989955	-1.571542	3.911309	0.000676	0.719600
-3.601501	-1.623968	3.921306	0.000603	0.719634
-3.274048	-1.547541	3.931302	0.000542	0.719900
-2.858703	-1.623709	3.941299	0.000464	0.719897
-2.966889	-1.604024	3.951296	0.000484	0.719898
-2.688774	-1.528837	3.961293	0.000431	0.720145
-2.172478	-1.581037	3.971290	0.000335	0.720224
-2.082761	-1.599334	3.981286	0.000318	0.720220
-2.017573	-1.550198	3.991283	0.000305	0.720340
-1.722003	-1.503766	4.001280	0.000250	0.720536
-1.585711	-1.528610	4.011277	0.000224	0.720535
-1.246497	-1.539204	4.021274	0.000161	0.720634
-1.420477	-1.387466	4.031270	0.000192	0.720873
-1.040255	-1.454079	4.041267	0.000121	0.720876
-1.259145	-1.343651	4.051264	0.000162	0.721017
-0.915805	-1.351049	4.061261	0.000097	0.721123
-0.941749	-1.311676	4.071258	0.000102	0.721192
-0.574229	-1.253406	4.081254	0.000033	0.721436
-0.992013	-1.164598	4.091251	0.000110	0.721465
-0.754471	-1.064165	4.101248	0.000066	0.721747
-0.499394	-1.084546	4.111245	0.000018	0.721797
-0.715927	-0.905221	4.121242	0.000057	0.722074
-0.735797	-0.835923	4.131238	0.000061	0.722204
-0.659218	-0.766313	4.141235	0.000046	0.722368
-0.535792	-0.648843	4.151232	0.000023	0.722642
-0.453769	-0.582779	4.161229	0.000007	0.722801
-0.415322	-0.484796	4.171226	-0.000001	0.723008
-0.387612	-0.337444	4.181222	-0.000006	0.723307
-0.295046	-0.257873	4.191219	-0.000024	0.723496
-0.204376	-0.164739	4.201216	-0.000041	0.723711
-0.138468	-0.052723	4.211213	-0.000054	0.723954
-0.154906	0.102730	4.221210	-0.000052	0.724254
0.000000	0.220493	4.231206	-0.000081	0.724539

0.251358	0.813418	4.236211	-0.000128	0.725787
0.243530	2.088188	4.241216	-0.000128	0.728271
0.382586	3.931009	4.246221	-0.000155	0.731899
0.777120	6.285963	4.251226	-0.000230	0.736584
0.943967	9.184908	4.256230	-0.000263	0.742201
1.206646	12.557613	4.261235	-0.000315	0.748707
1.363750	16.391236	4.266240	-0.000347	0.755986
1.850051	20.568554	4.271245	-0.000440	0.763943
2.007035	25.218982	4.276250	-0.000473	0.772579
2.378777	30.182243	4.281254	-0.000545	0.781756
3.005612	35.454601	4.286259	-0.000666	0.791462
3.855370	41.009255	4.291264	-0.000828	0.801619
4.216786	46.956086	4.296269	-0.000899	0.812183
4.594226	53.184662	4.301274	-0.000974	0.823102
5.143491	59.653867	4.306278	-0.001080	0.834338
5.577854	66.355626	4.311283	-0.001166	0.845780
6.278322	73.243121	4.316288	-0.001301	0.857454
6.910844	80.349556	4.321293	-0.001423	0.869309
7.589547	87.640535	4.326298	-0.001555	0.881313
7.787497	95.180576	4.331302	-0.001597	0.893417
8.536453	102.783192	4.336307	-0.001741	0.905609
9.252198	110.554755	4.341312	-0.001880	0.917891
9.650670	118.474570	4.346317	-0.001959	0.930151
10.456895	126.445361	4.351322	-0.002115	0.942435
12.538126	134.305206	4.356326	-0.002508	0.954727
13.391438	142.478382	4.361331	-0.002672	0.967006
14.088393	150.780141	4.366336	-0.002808	0.979278
14.615978	159.190841	4.371341	-0.002911	0.991511
15.511458	167.584267	4.376346	-0.003084	1.003661
16.194178	176.047971	4.381350	-0.003217	1.015711
17.513295	184.438507	4.386355	-0.003468	1.027671
18.492218	192.951406	4.391360	-0.003656	1.039579
18.709957	201.607774	4.396365	-0.003702	1.051367
19.839521	210.137377	4.401370	-0.003919	1.063066
20.670299	218.764248	4.406374	-0.004079	1.074697
21.228821	227.412756	4.411379	-0.004189	1.086170
22.283804	236.009687	4.416384	-0.004391	1.097566
22.631195	244.720368	4.421389	-0.004462	1.108835
23.768464	253.299830	4.426394	-0.004679	1.119995
24.498936	261.945239	4.431398	-0.004821	1.131041
24.872897	270.646963	4.436403	-0.004897	1.141972
25.773921	279.287329	4.441408	-0.005070	1.152836
26.427626	287.916900	4.446413	-0.005198	1.163533
27.022861	296.563378	4.451418	-0.005314	1.174141
27.795672	305.145637	4.456422	-0.005464	1.184612
28.159720	313.808113	4.461427	-0.005538	1.195004
28.765023	322.400096	4.466432	-0.005656	1.205272
29.363344	330.984712	4.471437	-0.005773	1.215443
30.406336	339.484223	4.476442	-0.005973	1.225517
30.977107	348.079037	4.481446	-0.006085	1.235527
31.318383	356.649486	4.486451	-0.006155	1.245384
32.212336	365.148112	4.491456	-0.006327	1.255188
32.574241	373.689504	4.496461	-0.006400	1.264862
33.072723	382.234761	4.501466	-0.006499	1.274493
34.029399	390.658233	4.506470	-0.006682	1.284002
34.488867	399.176162	4.511475	-0.006774	1.293453
35.016128	407.660676	4.516480	-0.006878	1.302811
35.746841	416.183121	4.521485	-0.007019	1.312180
36.281764	424.668972	4.526490	-0.007125	1.321408
36.797343	433.081622	4.531494	-0.007226	1.330490
37.289004	441.498710	4.536499	-0.007324	1.339510
37.941503	449.884179	4.541504	-0.007451	1.348465
38.386835	458.294017	4.546509	-0.007539	1.357350
38.901985	466.672120	4.551514	-0.007641	1.366157
39.475285	475.056118	4.556518	-0.007753	1.374922
39.921454	483.425172	4.561523	-0.007842	1.383595
40.670769	491.779698	4.566528	-0.007987	1.392250
41.105657	500.130737	4.571533	-0.008074	1.400795
41.797711	508.453647	4.576538	-0.008208	1.409303
42.198557	516.823776	4.581542	-0.008289	1.417758
42.732854	525.136696	4.586547	-0.008394	1.426128
43.148583	533.500210	4.591552	-0.008477	1.434480
43.558178	541.806999	4.596557	-0.008559	1.442726
44.144154	550.111514	4.601562	-0.008673	1.450952
44.548534	558.432634	4.606566	-0.008754	1.459118
44.962592	566.737812	4.611571	-0.008837	1.467225
45.336800	575.118046	4.616576	-0.008912	1.475352
46.039622	583.331544	4.621581	-0.009049	1.483328
46.453781	591.625628	4.626586	-0.009132	1.491291
46.979109	599.887686	4.631590	-0.009235	1.499200
47.509780	608.139104	4.636595	-0.009339	1.507057
48.148148	616.407600	4.641600	-0.009464	1.514906
48.487385	624.671052	4.646605	-0.009533	1.522664
49.248674	632.888458	4.651610	-0.009680	1.530404
49.625947	641.168790	4.656614	-0.009756	1.538105
49.943955	649.432793	4.661619	-0.009820	1.545743
50.432826	657.701211	4.666624	-0.009917	1.553374
51.143530	665.879917	4.671629	-0.010055	1.560917
51.878102	674.083836	4.676634	-0.010197	1.568451
52.167094	682.365127	4.681638	-0.010257	1.575953
52.457495	690.607523	4.686643	-0.010316	1.583385
52.920490	698.844606	4.691648	-0.010408	1.590802
53.371366	707.062610	4.696653	-0.010498	1.598166
53.744607	715.282366	4.701658	-0.010573	1.605486
54.044134	723.533813	4.706662	-0.010634	1.612791
54.567776	731.723598	4.711667	-0.010737	1.620040
55.272306	739.900068	4.716672	-0.010874	1.627270
55.662327	748.173185	4.721677	-0.010952	1.634508
56.055283	756.363740	4.726682	-0.011031	1.641643
56.566505	764.537580	4.731686	-0.011131	1.648749
56.759491	772.766920	4.736691	-0.011173	1.655829
56.946345	780.987256	4.741696	-0.011213	1.662870
57.433865	789.149476	4.746701	-0.011309	1.669872
57.839672	797.351168	4.751706	-0.011391	1.676867
58.071007	805.535219	4.756710	-0.011439	1.683795
58.304074	813.733424	4.761715	-0.011488	1.690706
58.772682	821.917215	4.766720	-0.011581	1.697609
59.137529	830.079255	4.771725	-0.011654	1.704451
59.428151	838.291495	4.776730	-0.011714	1.711298
60.110162	846.421389	4.781734	-0.011846	1.718100
60.497221	854.564243	4.786739	-0.011924	1.724848
61.153932	862.718277	4.791744	-0.012052	1.731613
61.623999	870.870546	4.796749	-0.012145	1.738327
62.052868	879.028975	4.801754	-0.012230	1.745014
62.271076	887.236087	4.806758	-0.012276	1.751688
62.660625	895.391389	4.811763	-0.012354	1.758317
63.301093	903.498663	4.816768	-0.012479	1.764913
63.337233	911.715856	4.821773	-0.012491	1.771498
63.709521	919.889041	4.826778	-0.012566	1.778064
64.093498	928.026881	4.831782	-0.012643	1.784580
64.455697	936.211876	4.836787	-0.012716	1.791106
65.001395	944.371118	4.841792	-0.012823	1.797611
65.331372	952.490036	4.846797	-0.012890	1.804034
65.866071	960.608381	4.851802	-0.012995	1.810459
66.314076	968.759876	4.856806	-0.013084	1.816876
66.712144	976.886027	4.861811	-0.013164	1.823244
67.296584	985.010881	4.866816	-0.013278	1.829612
67.612158	993.171156	4.871821	-0.013343	1.835953
67.841587	1001.317947	4.876826	-0.013391	1.842251
68.404970	1009.424300	4.881830	-0.013501	1.848536
68.992622	1017.540960	4.886835	-0.013616	1.854811
69.493176	1025.678686	4.891840	-0.013715	1.861069
69.807512	1033.826011	4.896845	-0.013779	1.867293
70.135570	1042.019812	4.901850	-0.013845	1.873532
70.208749	1050.176672	4.906854	-0.013865	1.879694
70.585492	1058.270713	4.911859	-0.013940	1.885822
71.012391	1066.411991	4.916864	-0.014025	1.891972
71.230551	1074.548439	4.921869	-0.014071	1.898075
71.806109	1082.632319	4.926874	-0.014184	1.904159
72.257931	1090.767227	4.931878	-0.014274	1.910248
72.493418	1098.912417	4.936883	-0.014323	1.916300
72.868726	1107.032791	4.941888	-0.014398	1.922331
73.179099	1115.144581	4.946893	-0.014462	1.928329
73.747986	1123.255775	4.951898	-0.014573	1.934336
74.252104	1131.353873	4.956902	-0.014672	1.940308
74.547641	1139.475451	4.961907	-0.014733	1.946256
74.812433	1147.670258	4.966912	-0.014788	1.952236
75.026149	1155.794650	4.971917	-0.014833	1.958140
75.411651	1163.871271	4.976922	-0.014910	1.964011
76.216575	1171.906891	4.981926	-0.015065	1.969880
76.374169	1180.053347	4.986931	-0.015100	1.975742
76.733747	1188.167594	4.991936	-0.015173	1.981584
77.015317	1196.256351	4.996941	-0.015231	1.987383
77.285431	1204.420157	5.001946	-0.015286	1.993217
77.420696	1212.544590	5.006950	-0.015317	1.998992
77.679890	1220.626511	5.011955	-0.015371	2.004733
78.160738	1228.720961	5.016960	-0.015466	2.010489
78.520909	1236.828409	5.021965	-0.015538	2.016226
78.672910	1244.956111	5.026970	-0.015572	2.021938
79.026636	1253.054600	5.031974	-0.015644	2.027635
79.475060	1261.170298	5.036979	-0.015733	2.033338
79.850426	1269.265034	5.041984	-0.015808	2.039003
80.005934	1277.348822	5.046989	-0.015842	2.044621
80.408951	1285.445363	5.051994	-0.015923	2.050259
80.648881	1293.573005	5.056998	-0.015973	2.055885
80.983621	1301.638986	5.062003	-0.016041	2.061464
81.830343	1309.674857	5.067008	-0.016204	2.067058
81.984779	1317.810435	5.072013	-0.016238	2.072635
82.376226	1325.914042	5.077018	-0.016316	2.078200
82.661121	1334.014516	5.082022	-0.016375	2.083736
82.888747	1342.113065	5.087027	-0.016423	2.089251
83.234043	1350.241549	5.092032	-0.016493	2.094783
83.111400	1358.373215	5.097037	-0.016475	2.100257
83.674963	1366.416701	5.102042	-0.016586	2.105725
84.183069	1374.535675	5.107046	-0.016686	2.111223
84.690240	1382.629892	5.112051	-0.016786	2.116690
85.111218	1390.700043	5.117056	-0.016870	2.122118
85.325812	1398.779366	5.122061	-0.016915	2.127519
85.637245	1406.880301	5.127066	-0.016978	2.132930
85.923684	1414.964366	5.132070	-0.017037	2.138314
85.993916	1423.061486	5.137075	-0.017056	2.143672
86.458907	1431.144700	5.142080	-0.017148	2.149044
86.589028	1439.265966	5.147085	-0.017178	2.154397
87.171837	1447.282385	5.152090	-0.017291	2.159710
87.636793	1455.353236	5.157094	-0.017384	2.165034
88.010590	1463.418747	5.162099	-0.017459	2.170334
88.383525	1471.536072	5.167104	-0.017533	2.175653
88.682198	1479.601809	5.172109	-0.017595	2.180920
88.950065	1487.700332	5.177114	-0.017650	2.186192
89.552633	1495.782826	5.182118	-0.017768	2.191472
89.631513	1503.914487	5.187123	-0.017788	2.196722
90.041517	1511.972272	5.192128	-0.017870	2.201943
90.284961	1520.044489	5.197133	-0.017920	2.207146
90.564441	1528.146737	5.202138	-0.017978	2.212358
90.952106	1536.213460	5.207142	-0.018055	2.217546
91.176390	1544.284296	5.212147	-0.018103	2.222709
91.652205	1552.355272	5.217152	-0.018197	2.227883
91.992929	1560.448268	5.222157	-0.018266	2.233046
92.193904	1568.528430	5.227162	-0.018309	2.238177
92.594117	1576.587835	5.232166	-0.018389	2.243301
92.901515	1584.653354	5.237171	-0.018451	2.248408
93.321190	1592.747672	5.242176	-0.018535	2.253532
93.320633	1600.856105	5.247181	-0.018540	2.258617
93.852535	1608.890401	5.252186	-0.018645	2.263689
94.058329	1616.987827	5.257190	-0.018688	2.268762
94.107883	1625.169329	5.262195	-0.018703	2.273862
94.741243	1633.181647	5.267200	-0.018827	2.278895
95.023695	1641.201864	5.272205	-0.018885	2.283893
95.191853	1649.299818	5.277210	-0.018921	2.288917
95.612965	1657.378337	5.282214	-0.019005	2.293940
95.939889	1665.415262	5.287219	-0.019072	2.298918
96.286001	1673.486535	5.292224	-0.019141	2.303909
96.292249	1681.589285	5.297229	-0.019148	2.308879
96.675444	1689.666334	5.302234	-0.019225	2.313854
96.966749	1697.722683	5.307238	-0.019285	2.318798
97.280323	1705.761855	5.312243	-0.019348	2.323723
97.618273	1713.839144	5.317248	-0.019417	2.328663
97.876039	1721.921306	5.322253	-0.019470	2.333588
98.123198	1729.991204	5.327258	-0.019522	2.338495
98.452553	1738.050265	5.332262	-0.019589	2.343391
98.737798	1746.118141	5.337267	-0.019647	2.348279
99.122902	1754.226137	5.342272	-0.019724	2.353189
99.179275	1762.296870	5.347277	-0.019740	2.358040
99.324044	1770.353828	5.352282	-0.019773	2.362880
99.830868	1778.377059	5.357286	-0.019872	2.367718
100.135927	1786.435036	5.362291	-0.019935	2.372551
100.516669	1794.514973	5.367296	-0.020011	2.377394
100.709974	1802.572905	5.372301	-0.020052	2.382198
101.049871	1810.640252	5.377306	-0.020121	2.387010
101.485759	1818.709164	5.382310	-0.020208	2.391821
101.928486	1826.751649	5.387315	-0.020296	2.396607
102.344024	1834.805924	5.392320	-0.020379	2.401388
102.580562	1842.873285	5.397325	-0.020428	2.406153
102.820988	1850.960014	5.402330	-0.020478	2.410920
103.132824	1859.039572	5.407334	-0.020542	2.415679
103.270605	1867.105726	5.412339	-0.020573	2.420408
103.407057	1875.188466	5.417344	-0.020604	2.425136
103.754243	1883.250373	5.422349	-0.020674	2.429860
103.863222	1891.412857	5.427354	-0.020700	2.434615
104.250880	1899.416252	5.432358	-0.020777	2.439289
104.631123	1907.416002	5.437363	-0.020853	2.443951
104.864557	1915.485174	5.442368	-0.020902	2.448634
104.986915	1923.556365	5.447373	-0.020931	2.453300
105.180975	1931.621137	5.452378	-0.020972	2.457959
105.580452	1939.653268	5.457382	-0.021052	2.462606
105.503141	1947.739428	5.462387	-0.021043	2.467240
106.077546	1955.774841	5.467392	-0.021155	2.471884
106.266782	1963.832989	5.472397	-0.021196	2.476504
106.477032	1971.890435	5.477402	-0.021241	2.481116
106.810200	1979.934160	5.482406	-0.021308	2.485721
107.118124	1987.989699	5.487411	-0.021371	2.490322
107.543451	1996.069103	5.492416	-0.021456	2.494937
107.726100	2004.115372	5.497421	-0.021495	2.499507
107.910106	2012.163602	5.502426	-0.021535	2.504069
108.374753	2020.232561	5.507430	-0.021627	2.508655
108.606672	2028.337937	5.512435	-0.021675	2.513237
108.912923	2036.388669	5.517440	-0.021738	2.517784
109.124485	2044.426766	5.522445	-0.021783	2.522310
109.205237	2052.480297	5.527450	-0.021803	2.526827
109.439105	2060.552467	5.532454	-0.021852	2.531356
109.792024	2068.574497	5.537459	-0.021923	2.535859
110.144400	2076.654271	5.542464	-0.021994	2.540385
110.366368	2084.683528	5.547469	-0.022041	2.544866
110.560411	2092.749209	5.552474	-0.022083	2.549357
110.925635	2100.818512	5.557478	-0.022156	2.553854
110.971377	2108.863392	5.562483	-0.022170	2.558308
111.398077	2116.879785	5.567488	-0.022255	2.562764
111.501711	2124.956602	5.572493	-0.022280	2.567224
111.863491	2133.014405	5.577498	-0.022353	2.571683
112.168601	2141.065405	5.582502	-0.022415	2.576126
112.357937	2149.098904	5.587507	-0.022456	2.580545
112.903680	2157.119529	5.592512	-0.022563	2.584973
113.076592	2165.197268	5.597517	-0.022600	2.589399
113.307177	2173.459001	5.602522	-0.022649	2.593922
113.635171	2181.454032	5.607526	-0.022715	2.598299
113.867169	2189.443117	5.612531	-0.022764	2.602658
114.180620	2197.461503	5.617536	-0.022828	2.607031
114.414392	2205.505192	5.622541	-0.022877	2.611405
114.851487	2213.541888	5.627546	-0.022963	2.615782
114.876227	2221.602941	5.632550	-0.022973	2.620137
115.169866	2229.611686	5.637555	-0.023034	2.624474
115.452988	2237.683637	5.642560	-0.023092	2.628838
115.576199	2245.747045	5.647565	-0.023120	2.633179
115.787179	2253.783031	5.652570	-0.023165	2.637504
116.248831	2261.794796	5.657574	-0.023256	2.641825
116.240272	2269.852292	5.662579	-0.023260	2.646133
116.398509	2277.942271	5.667584	-0.023295	2.650462
116.556983	2286.009495	5.672589	-0.023330	2.654772
116.831252	2294.028503	5.677594	-0.023386	2.659056
117.071198	2302.074805	5.682598	-0.023437	2.663346
117.106836	2310.128488	5.687603	-0.023449	2.667620
117.517212	2318.186705	5.692608	-0.023531	2.671913
117.631227	2326.253937	5.697613	-0.023557	2.676185
117.964306	2334.263174	5.702618	-0.023625	2.680434
118.180786	2342.292323	5.707622	-0.023670	2.684679
118.453940	2350.307868	5.712627	-0.023727	2.688914
118.482981	2358.427533	5.717632	-0.023738	2.693181
118.717510	2366.449558	5.722637	-0.023787	2.697403
119.032257	2374.479422	5.727642	-0.023851	2.701628
119.226993	2382.530482	5.732646	-0.023892	2.705849
119.251547	2390.611049	5.737651	-0.023902	2.710069
119.646349	2398.650324	5.742656	-0.023981	2.714284
119.568018	2406.713240	5.747661	-0.023972	2.718475
119.851674	2414.703883	5.752666	-0.024030	2.722644
120.121311	2422.773660	5.757670	-0.024086	2.726847
120.557854	2430.788551	5.762675	-0.024173	2.731026
120.971920	2438.859122	5.767680	-0.024255	2.735225
121.110640	2446.907816	5.772685	-0.024287	2.739390
121.520996	2454.927008	5.777690	-0.024369	2.743550
121.601837	2463.003610	5.782694	-0.024389	2.747713
121.830472	2471.107908	5.787699	-0.024437	2.751892
122.066459	2479.211017	5.792704	-0.024486	2.756066
122.303757	2487.194098	5.797709	-0.024536	2.760171
122.632332	2495.180327	5.802714	-0.024603	2.764277
123.024894	2503.219436	5.807718	-0.024681	2.768408
123.210055	2511.263197	5.812723	-0.024721	2.772523
123.570045	2519.308420	5.817728	-0.024794	2.776643
123.897007	2527.313757	5.822733	-0.024860	2.780734
124.047436	2535.344240	5.827738	-0.024893	2.784822
124.120287	2543.435671	5.832742	-0.024912	2.788930
124.387975	2551.482550	5.837747	-0.024968	2.793021
124.813767	2559.518753	5.842752	-0.025052	2.797109
125.232374	2567.519527	5.847757	-0.025136	2.801173
125.394251	2575.553735	5.852762	-0.025171	2.805234
125.539701	2583.622052	5.857766	-0.025204	2.809304
125.840792	2591.679910	5.862771	-0.025265	2.813372
126.358176	2599.711705	5.867776	-0.025367	2.817434
126.332237	2607.772163	5.872781	-0.025368	2.821473
126.443518	2615.812234	5.877786	-0.025394	2.825504
126.692373	2623.865643	5.882790	-0.025446	2.829543
126.706918	2631.961183	5.887795	-0.025454	2.833585
127.341610	2639.943163	5.892800	-0.025577	2.837599
127.642240	2647.967863	5.897805	-0.025639	2.841610
127.691112	2656.020693	5.902810	-0.025653	2.845615
128.207559	2664.028170	5.907814	-0.025755	2.849618
128.417254	2672.098271	5.912819	-0.025799	2.853629
128.773037	2680.121696	5.917824	-0.025871	2.857620
128.767578	2688.187758	5.922829	-0.025876	2.861605
129.015400	2696.203031	5.927834	-0.025927	2.865575
129.518038	2704.233916	5.932838	-0.026026	2.869560
129.360796	2712.319738	5.937843	-0.026002	2.873531
129.707871	2720.360875	5.942848	-0.026072	2.877502
129.873363	2728.391583	5.947853	-0.026109	2.881452
130.021106	2736.407340	5.952858	-0.026142	2.885389
130.328723	2744.468043	5.957862	-0.026204	2.889350
130.698124	2752.500520	5.962867	-0.026278	2.893296
130.861229	2760.558091	5.967872	-0.026314	2.897238
131.070299	2768.597284	5.972877	-0.026359	2.901167
131.435247	2776.591760	5.977882	-0.026432	2.905078
131.681567	2784.669431	5.982886	-0.026483	2.909018
131.877374	2792.766331	5.987891	-0.026525	2.912959
132.182763	2800.835197	5.992896	-0.026588	2.916887
132.223504	2808.834447	5.997901	-0.026601	2.920761
132.387767	2816.823063	6.002906	-0.026637	2.924632
132.752622	2824.859305	6.007910	-0.026710	2.928532
132.989953	2832.885394	6.012915	-0.026760	2.932414
133.395859	2840.940867	6.017920	-0.026841	2.936315
133.289233	2848.974022	6.022925	-0.026826	2.940172
133.682809	2856.974428	6.027930	-0.026905	2.944035
134.124964	2865.025238	6.032934	-0.026993	2.947919
134.218623	2873.084826	6.037939	-0.027016	2.951785
134.364236	2881.177509	6.042944	-0.027048	2.955664
134.598005	2889.151082	6.047949	-0.027097	2.959485
134.946829	2897.152832	6.052954	-0.027167	2.963321
135.114803	2905.226526	6.057958	-0.027204	2.967176
135.284770	2913.258743	6.062963	-0.027241	2.971007
135.539538	2921.325217	6.067968	-0.027294	2.974854
135.448480	2929.368130	6.072973	-0.027283	2.978667
135.796771	2937.361283	6.077978	-0.027353	2.982473
136.237961	2945.407083	6.082982	-0.027440	2.986305
136.426481	2953.407706	6.087987	-0.027481	2.990097
136.745649	2961.521839	6.092992	-0.027546	2.993945
137.074564	2969.515718	6.097997	-0.027613	2.997731
137.345212	2977.517417	6.103002	-0.027668	3.001513
137.144653	2985.610261	6.108006	-0.027636	3.005310
137.419572	2993.604680	6.113011	-0.027693	3.009080
137.841451	3001.651092	6.118016	-0.027777	3.012876
137.968499	3009.707468	6.123021	-0.027806	3.016658
138.014479	3017.747805	6.128026	-0.027820	3.020423
138.434867	3025.756416	6.133030	-0.027904	3.024188
138.499281	3033.788265	6.138035	-0.027921	3.027940
138.817133	3041.855328	6.143040	-0.027986	3.031717
139.275517	3049.883814	6.148045	-0.028077	3.035479
139.710449	3057.853740	6.153050	-0.028163	3.039207
139.991404	3065.923594	6.158054	-0.028221	3.042969
140.174231	3073.949087	6.163059	-0.028260	3.046701
140.574289	3082.002575	6.168064	-0.028340	3.050452
140.830448	3090.053325	6.173069	-0.028393	3.054191
140.876012	3098.093136	6.178074	-0.028407	3.057909
141.400449	3106.111937	6.183078	-0.028510	3.061636
141.493215	3114.131441	6.188083	-0.028533	3.065339
141.959088	3122.157181	6.193088	-0.028625	3.069057
142.018431	3130.298180	6.198093	-0.028642	3.072805
142.364882	3138.311834	6.203098	-0.028712	3.076503
142.608348	3146.310373	6.208102	-0.028762	3.080184
142.328578	3154.339613	6.213107	-0.028716	3.083851
142.555288	3162.391183	6.218112	-0.028763	3.087548
142.818194	3170.419494	6.223117	-0.028818	3.091231
142.892756	3178.460084	6.228122	-0.028837	3.094906
143.057066	3186.491664	6.233126	-0.028873	3.098578
143.233239	3194.472018	6.238131	-0.028911	3.102222
143.552935	3202.506509	6.243136	-0.028976	3.105893
143.816756	3210.531520	6.248141	-0.029031	3.109552
144.243061	3218.585692	6.253146	-0.029116	3.113228
144.543403	3226.633220	6.258150	-0.029177	3.116891
144.826668	3234.649309	6.263155	-0.029235	3.120534
144.970277	3242.652175	6.268160	-0.029267	3.124161
145.129629	3250.723007	6.273165	-0.029302	3.127815
145.089122	3258.769129	6.278170	-0.029300	3.131445
145.464742	3266.820951	6.283174	-0.029376	3.135091
145.729161	3274.821140	6.288179	-0.029430	3.138705
145.850292	3282.861436	6.293184	-0.029458	3.142327
146.120461	3290.891596	6.298189	-0.029514	3.145946
146.349913	3298.885703	6.303194	-0.029562	3.149543
146.718195	3306.987032	6.308198	-0.029636	3.153190
146.774624	3315.013888	6.313203	-0.029652	3.156786
146.873977	3323.037375	6.318208	-0.029676	3.160378
147.128151	3331.045228	6.323213	-0.029729	3.163966
147.227307	3339.046515	6.328218	-0.029753	3.167540
147.647972	3347.099415	6.333222	-0.029837	3.171147
147.869695	3355.119841	6.338227	-0.029883	3.174727
148.148768	3363.147429	6.343232	-0.029941	3.178308
148.274515	3371.189807	6.348237	-0.029970	3.181885
148.661911	3379.200724	6.353242	-0.030047	3.185455
148.698748	3387.274821	6.358246	-0.030059	3.189035
148.789176	3395.307024	6.363251	-0.030082	3.192594
149.011567	3403.383709	6.368256	-0.030129	3.196174
149.264367	3411.369065	6.373261	-0.030181	3.199711
149.376036	3419.365456	6.378266	-0.030207	3.203244
149.605711	3427.438246	6.383270	-0.030255	3.206811
149.909856	3435.439297	6.388275	-0.030317	3.210345
149.947938	3443.513500	6.393280	-0.030330	3.213897
150.253253	3451.535939	6.398285	-0.030392	3.217433
150.484431	3459.545845	6.403290	-0.030441	3.220956
150.714900	3467.567560	6.408294	-0.030489	3.224481
150.843819	3475.601966	6.413299	-0.030519	3.228003
151.106816	3483.679137	6.418304	-0.030573	3.231546
151.244053	3491.743411	6.423309	-0.030604	3.235073
151.516928	3499.711593	6.428314	-0.030660	3.238561
151.637782	3507.744897	6.433318	-0.030688	3.242067
151.959535	3515.726747	6.438323	-0.030753	3.245555
152.051198	3523.739324	6.443328	-0.030776	3.249043
152.368017	3531.794455	6.448333	-0.030840	3.252555
152.677722	3539.838955	6.453338	-0.030903	3.256058
152.917750	3547.831654	6.458342	-0.030954	3.259533
153.162232	3555.847026	6.463347	-0.031004	3.263013
153.360816	3563.925108	6.468352	-0.031047	3.266515
153.615017	3571.955561	6.473357	-0.031100	3.269995
153.569305	3580.032854	6.478362	-0.031097	3.273479
153.932569	3588.044643	6.483366	-0.031170	3.276948
154.203680	3596.026313	6.488371	-0.031226	3.280396
154.451757	3604.054906	6.493376	-0.031277	3.283860
154.558296	3612.106330	6.498381	-0.031302	3.287324
154.763601	3620.135586	6.503386	-0.031346	3.290779
155.064723	3628.180802	6.508390	-0.031408	3.294241
155.344153	3636.181166	6.513395	-0.031465	3.297680
155.471341	3644.245976	6.518400	-0.031494	3.301136
155.655253	3652.227297	6.523405	-0.031534	3.304555
155.965397	3660.251083	6.528410	-0.031597	3.307994
156.188278	3668.352633	6.533414	-0.031644	3.311459
156.405298	3676.380482	6.538419	-0.031690	3.314888
156.549010	3684.399030	6.543424	-0.031722	3.318307
156.638902	3692.419661	6.548429	-0.031744	3.321722
156.877555	3700.397258	6.553434	-0.031794	3.325120
157.086869	3708.449011	6.558438	-0.031838	3.328545
157.081033	3716.484569	6.563443	-0.031843	3.331952
157.400709	3724.543380	6.568448	-0.031908	3.335377
157.719460	3732.547965	6.573453	-0.031972	3.338776
157.721474	3740.575160	6.578458	-0.031978	3.342169
158.018078	3748.582692	6.583462	-0.032039	3.345561
158.227486	3756.629760	6.588467	-0.032083	3.348963
158.384440	3764.685951	6.593472	-0.032118	3.352363
158.629853	3772.730894	6.598477	-0.032169	3.355759
158.805352	3780.698028	6.603482	-0.032207	3.359116
159.237449	3788.710647	6.608486	-0.032293	3.362497
159.208086	3796.742841	6.613491	-0.032293	3.365867
159.483375	3804.777124	6.618496	-0.032350	3.369246
159.790917	3812.825805	6.623501	-0.032412	3.372628
159.930234	3820.876146	6.628506	-0.032444	3.376001
160.077847	3828.876366	6.633510	-0.032477	3.379350
160.281679	3836.888810	6.638515	-0.032520	3.382703
160.615063	3844.953009	6.643520	-0.032588	3.386079
160.639625	3852.967539	6.648525	-0.032598	3.389420
160.827866	3861.048239	6.653530	-0.032638	3.392791
161.279205	3869.105958	6.658534	-0.032728	3.396158
161.384588	3877.049785	6.663539	-0.032753	3.399462
161.558518	3885.046083	6.668544	-0.032790	3.402787
161.629113	3893.089796	6.673549	-0.032809	3.406126
161.835017	3901.086448	6.678554	-0.032853	3.409445
162.076676	3909.167275	6.683558	-0.032903	3.412798
162.413543	3917.164425	6.688563	-0.032971	3.416116
162.686198	3925.161969	6.693568	-0.033028	3.419429
162.737198	3933.205359	6.698573	-0.033042	3.422750
162.948236	3941.243429	6.703578	-0.033087	3.426071
163.197922	3949.268789	6.708582	-0.033139	3.429384
163.388549	3957.311425	6.713587	-0.033180	3.432700
163.342572	3965.382019	6.718592	-0.033177	3.436016
163.661296	3973.364505	6.723597	-0.033242	3.439305
163.676611	3981.393916	6.728602	-0.033250	3.442599
163.990992	3989.423548	6.733606	-0.033314	3.445901
164.314689	3997.400018	6.738611	-0.033380	3.449178
164.566851	4005.458725	6.743616	-0.033432	3.452483
164.727766	4013.517339	6.748621	-0.033467	3.455781
164.822058	4021.493458	6.753626	-0.033490	3.459041
165.188095	4029.562587	6.758630	-0.033564	3.462344
165.097864	4037.571056	6.763635	-0.033553	3.465605
165.297214	4045.617651	6.768640	-0.033595	3.468887
165.686855	4053.660673	6.773645	-0.033673	3.472171
165.730883	4061.697411	6.778650	-0.033687	3.475439
165.900208	4069.703355	6.783654	-0.033724	3.478694
165.996802	4077.699523	6.788659	-0.033747	3.481941
166.422493	4085.693476	6.793664	-0.033832	3.485193
166.366280	4093.750705	6.798669	-0.033827	3.488453
166.589058	4101.780460	6.803674	-0.033874	3.491708
167.125091	4109.794878	6.808678	-0.033979	3.494963
167.141446	4117.796420	6.813683	-0.033987	3.498194
167.318109	4125.850214	6.818688	-0.034026	3.501448
167.413799	4133.857407	6.823693	-0.034049	3.504677
167.613041	4141.882645	6.828698	-0.034091	3.507914
167.724937	4149.964074	6.833702	-0.034118	3.511168
167.861294	4157.961782	6.838707	-0.034149	3.514386
168.081663	4165.961216	6.843712	-0.034195	3.517604
168.369484	4173.985500	6.848717	-0.034254	3.520831
168.429857	4181.952042	6.853722	-0.034271	3.524025
168.894056	4190.029259	6.858726	-0.034363	3.527273
168.955091	4198.079978	6.863731	-0.034379	3.530495
169.417442	4206.120161	6.868736	-0.034471	3.533722
169.689987	4214.141586	6.873741	-0.034527	3.536932
169.734649	4222.146905	6.878746	-0.034541	3.540127
169.789562	4230.206521	6.883750	-0.034556	3.543340
169.899932	4238.222255	6.888755	-0.034582	3.546535
170.281436	4246.254815	6.893760	-0.034659	3.549742
170.628547	4254.383056	6.898765	-0.034729	3.552982
170.626570	4262.393844	6.903770	-0.034734	3.556163
170.880693	4270.341612	6.908774	-0.034787	3.559323
171.024873	4278.353569	6.913779	-0.034819	3.562503
171.189226	4286.357859	6.918784	-0.034855	3.565678
171.414804	4294.388536	6.923789	-0.034902	3.568861
171.624938	4302.407875	6.928794	-0.034947	3.572038
171.893021	4310.457888	6.933798	-0.035002	3.575224
172.166416	4318.441998	6.938803	-0.035059	3.578383
172.583926	4326.445763	6.943808	-0.035142	3.581550
172.755004	4334.474728	6.948813	-0.035179	3.584717
172.935113	4342.483239	6.953818	-0.035218	3.587874
173.037645	4350.590299	6.958822	-0.035243	3.591064
173.469955	4358.564749	6.963827	-0.035329	3.594209
173.453472	4366.603339	6.968832	-0.035331	3.597364
173.598475	4374.627046	6.973837	-0.035363	3.600514
173.796035	4382.582343	6.978842	-0.035405	3.603636
173.983252	4390.663466	6.983846	-0.035446	3.606805
174.199551	4398.650688	6.988851	-0.035491	3.609935
174.347088	4406.717769	6.993856	-0.035524	3.613091
174.725915	4414.762811	6.998861	-0.035600	3.616242
174.858847	4422.721102	7.003866	-0.035631	3.619350
175.109044	4430.795054	7.008870	-0.035683	3.622504
175.233137	4438.793570	7.013875	-0.035711	3.625622
175.318432	4446.829046	7.018880	-0.035732	3.628750
175.540464	4454.899725	7.023885	-0.035779	3.631893
175.642449	4462.908653	7.028890	-0.035804	3.635007
175.782021	4470.934771	7.033894	-0.035835	3.638125
175.867109	4478.973227	7.038899	-0.035856	3.641244
176.170358	4486.919711	7.043904	-0.035918	3.644330
176.520977	4494.962616	7.048909	-0.035989	3.647453
176.546804	4502.986406	7.053914	-0.035999	3.650556
176.639354	4511.056129	7.058918	-0.036022	3.653677
176.902090	4519.058081	7.063923	-0.036076	3.656773
177.119460	4527.079743	7.068928	-0.036122	3.659873
177.044202	4535.121681	7.073933	-0.036113	3.662970
177.392777	4543.112527	7.078938	-0.036184	3.666056
177.794822	4551.140758	7.083942	-0.036264	3.669155
177.463512	4559.205790	7.088947	-0.036208	3.672247
177.971909	4567.208151	7.093952	-0.036308	3.675334
178.175071	4575.213470	7.098957	-0.036351	3.678411
178.234075	4583.241719	7.103962	-0.036368	3.681491
178.363628	4591.233717	7.108966	-0.036397	3.684556
178.688083	4599.281526	7.113971	-0.036463	3.687645
178.783150	4607.328532	7.118976	-0.036486	3.690725
179.081248	4615.373016	7.123981	-0.036547	3.693807
179.349621	4623.347785	7.128986	-0.036602	3.696859
179.684601	4631.360110	7.133990	-0.036670	3.699924
179.614834	4639.367980	7.138995	-0.036663	3.702975
179.765607	4647.445972	7.144000	-0.036696	3.706055
180.076930	4655.413643	7.149005	-0.036759	3.709095
180.126287	4663.484628	7.154010	-0.036774	3.712165
180.549839	4671.573526	7.159014	-0.036858	3.715249
180.769915	4679.536801	7.164019	-0.036905	3.718277
180.942939	4687.552510	7.169024	-0.036942	3.721322
181.143200	4695.533568	7.174029	-0.036985	3.724351
181.106673	4703.565184	7.179034	-0.036984	3.727392
181.317612	4711.594224	7.184038	-0.037028	3.730435
181.662041	4719.609070	7.189043	-0.037098	3.733473
181.592118	4727.642724	7.194048	-0.037090	3.736506
182.004492	4735.654163	7.199053	-0.037173	3.739540
182.290138	4743.656236	7.204058	-0.037231	3.742564
182.576298	4751.679803	7.209062	-0.037290	3.745595
182.412143	4759.742245	7.214067	-0.037265	3.748626
183.175224	4767.722760	7.219072	-0.037412	3.751647
183.215522	4775.792253	7.224077	-0.037425	3.754681
183.245874	4783.795738	7.229082	-0.037436	3.757688
183.540269	4791.854298	7.234086	-0.037497	3.760719
183.577398	4799.811196	7.239091	-0.037509	3.763704
183.710520	4807.883588	7.244096	-0.037539	3.766731
183.994735	4815.901598	7.249101	-0.037597	3.769740
183.984449	4823.917343	7.254106	-0.037601	3.772738
184.157387	4831.987683	7.259110	-0.037639	3.775758
184.412313	4839.956756	7.264115	-0.037691	3.778741
184.933784	4847.969746	7.269120	-0.037794	3.781743
185.184070	4855.984685	7.274125	-0.037846	3.784737
185.257300	4864.024231	7.279130	-0.037865	3.787734
185.648421	4872.082257	7.284134	-0.037943	3.790743
185.752676	4880.108511	7.289139	-0.037968	3.793731
185.635269	4888.164368	7.294144	-0.037952	3.796723
186.016827	4896.102875	7.299149	-0.038028	3.799680
186.219146	4904.135717	7.304154	-0.038071	3.802665
186.353821	4912.119982	7.309158	-0.038102	3.805629
186.540898	4920.151301	7.314163	-0.038142	3.808609
186.833907	4928.190417	7.319168	-0.038202	3.811592
187.143808	4936.242581	7.324173	-0.038265	3.814577
187.196984	4944.199468	7.329178	-0.038280	3.817520
187.437345	4952.250650	7.334182	-0.038331	3.820499
187.762445	4960.222964	7.339187	-0.038397	3.823448
187.802769	4968.300053	7.344192	-0.038410	3.826428
188.252331	4976.296518	7.349197	-0.038499	3.829384
188.428946	4984.353075	7.354202	-0.038537	3.832354
188.753138	4992.349021	7.359206	-0.038603	3.835303
188.752946	5000.366213	7.364211	-0.038608	3.838250
189.086772	5008.390307	7.369216	-0.038676	3.841205
189.129597	5016.392829	7.374221	-0.038689	3.844143
189.239687	5024.413914	7.379226	-0.038715	3.847088
189.490418	5032.440173	7.384230	-0.038767	3.850035
189.584673	5040.520623	7.389235	-0.038790	3.852996
189.588791	5048.530397	7.394240	-0.038796	3.855927
189.923647	5056.529732	7.399245	-0.038864	3.858859
190.292866	5064.524010	7.404250	-0.038938	3.861787
190.349718	5072.564736	7.409254	-0.038954	3.864724
190.429130	5080.623219	7.414259	-0.038975	3.867666
190.689020	5088.652359	7.419264	-0.039028	3.870598
190.912570	5096.884305	7.424269	-0.039076	3.873601
190.970221	5104.872572	7.429274	-0.039092	3.876510
191.209221	5112.777253	7.434278	-0.039142	3.879390
191.465784	5120.723925	7.439283	-0.039195	3.882283
191.674365	5128.753165	7.444288	-0.039239	3.885203
192.019144	5136.761498	7.449293	-0.039309	3.888116
192.012782	5144.779113	7.454298	-0.039313	3.891023
192.125999	5152.838644	7.459302	-0.039339	3.893945
192.086358	5160.846779	7.464307	-0.039337	3.896844
192.356164	5168.816148	7.469312	-0.039393	3.899733
192.584095	5176.870621	7.474317	-0.039441	3.902649
192.805567	5184.858076	7.479322	-0.039488	3.905539
193.019085	5192.898681	7.484326	-0.039533	3.908445
193.207404	5200.934552	7.489331	-0.039573	3.911347
193.238987	5208.971551	7.494336	-0.039585	3.914245
193.420578	5216.983421	7.499341	-0.039624	3.917134
193.540420	5224.954117	7.504346	-0.039651	3.920005
193.781154	5232.981007	7.509350	-0.039702	3.922896
193.704768	5240.970914	7.514355	-0.039693	3.925766
193.926847	5249.002008	7.519360	-0.039740	3.928655
194.329338	5257.052666	7.524365	-0.039820	3.931551
194.247900	5265.067501	7.529370	-0.039810	3.934423
194.471689	5273.092975	7.534374	-0.039857	3.937303
194.664712	5281.079728	7.539379	-0.039899	3.940166
194.834108	5289.098864	7.544384	-0.039936	3.943039
194.800957	5297.150519	7.549389	-0.039935	3.945917
195.144597	5305.132706	7.554394	-0.040004	3.948775
195.462316	5313.207829	7.559398	-0.040069	3.951663
195.319172	5321.244066	7.564403	-0.040048	3.954527
195.582013	5329.238325	7.569408	-0.040102	3.957382
195.803981	5337.252726	7.574413	-0.040149	3.960241
195.870461	5345.229624	7.579418	-0.040167	3.963081
196.018154	5353.270721	7.584422	-0.040200	3.965944
196.399016	5361.243296	7.589427	-0.040276	3.968785
196.625172	5369.280989	7.594432	-0.040323	3.971644
196.820783	5377.366502	7.599437	-0.040365	3.974517
196.942240	5385.339941	7.604442	-0.040393	3.977347
197.083580	5393.392202	7.609446	-0.040425	3.980203
197.216043	5401.387240	7.614451	-0.040455	3.983037
197.533500	5409.398826	7.619456	-0.040520	3.985878
197.801872	5417.437092	7.624461	-0.040575	3.988725
197.856040	5425.488473	7.629466	-0.040591	3.991571
198.147257	5433.541796	7.634470	-0.040650	3.994420
198.561513	5441.524560	7.639475	-0.040733	3.997244
198.857110	5449.520339	7.644480	-0.040793	4.000068
199.011862	5457.546913	7.649485	-0.040828	4.002899
199.204399	5465.567777	7.654490	-0.040869	4.005727
199.196990	5473.581219	7.659494	-0.040873	4.008547
199.370524	5481.638373	7.664499	-0.040911	4.011383
199.583075	5489.659572	7.669504	-0.040956	4.014205
199.862928	5497.688857	7.674509	-0.041013	4.017029
199.997092	5505.661836	7.679514	-0.041044	4.019829
200.169984	5513.737592	7.684518	-0.041081	4.022663
200.270814	5521.750985	7.689523	-0.041105	4.025473
200.281294	5529.735621	7.694528	-0.041113	4.028269
200.483390	5537.783530	7.699533	-0.041156	4.031088
200.701017	5545.889189	7.704538	-0.041202	4.033925
200.894435	5553.886400	7.709542	-0.041243	4.036723
201.005623	5561.799756	7.714547	-0.041269	4.039487
201.194040	5569.788680	7.719552	-0.041310	4.042278
201.234305	5577.819068	7.724557	-0.041323	4.045079
201.331431	5585.846365	7.729562	-0.041346	4.047877
201.518799	5593.922102	7.734566	-0.041387	4.050692
201.699075	5601.942809	7.739571	-0.041426	4.053486
201.901089	5609.943076	7.744576	-0.041469	4.056270
202.143705	5617.914889	7.749581	-0.041519	4.059044
202.320977	5625.940836	7.754586	-0.041558	4.061834
202.776399	5633.928532	7.759590	-0.041648	4.064612
202.552154	5641.962344	7.764595	-0.041611	4.067394
202.693035	5649.988487	7.769600	-0.041643	4.070178
203.010385	5658.068045	7.774605	-0.041708	4.072980
203.129449	5666.047599	7.779610	-0.041735	4.075743
203.294103	5674.063305	7.784614	-0.041771	4.078517
203.554757	5682.098780	7.789619	-0.041825	4.081298
203.464589	5690.074232	7.794624	-0.041814	4.084051
203.693782	5698.131072	7.799629	-0.041862	4.086834
203.630662	5706.103604	7.804634	-0.041856	4.089583
203.956495	5714.199438	7.809638	-0.041922	4.092377
204.127344	5722.219036	7.814643	-0.041959	4.095142
204.363681	5730.203476	7.819648	-0.042008	4.097893
204.605773	5738.227671	7.824653	-0.042059	4.100656
204.548228	5746.201662	7.829658	-0.042054	4.103396
204.743159	5754.249509	7.834662	-0.042095	4.106162
204.994486	5762.262510	7.839667	-0.042148	4.108916
205.392483	5770.287284	7.844672	-0.042227	4.111674
205.673315	5778.351188	7.849677	-0.042285	4.114441
205.449321	5786.373000	7.854682	-0.042249	4.117186
206.032349	5794.339895	7.859686	-0.042362	4.119921
206.076249	5802.349666	7.864691	-0.042376	4.122661
206.180576	5810.340639	7.869696	-0.042401	4.125394
206.308197	5818.412899	7.874701	-0.042430	4.128153
206.450248	5826.434291	7.879706	-0.042462	4.130893
206.639649	5834.497805	7.884710	-0.042503	4.133647
206.640434	5842.520460	7.889715	-0.042508	4.136382
206.719454	5850.496126	7.894720	-0.042528	4.139100
206.843669	5858.546089	7.899725	-0.042557	4.141843
206.970712	5866.528835	7.904730	-0.042586	4.144560
207.179881	5874.550719	7.909734	-0.042630	4.147291
207.595046	5882.535821	7.914739	-0.042713	4.150009
207.655238	5890.583803	7.919744	-0.042730	4.152743
207.839570	5898.665939	7.924749	-0.042770	4.155487
207.805375	5906.630283	7.929754	-0.042769	4.158188
207.920662	5914.671148	7.934758	-0.042795	4.160914
208.036636	5922.635251	7.939763	-0.042822	4.163613
208.283020	5930.668428	7.944768	-0.042874	4.166335
208.495777	5938.683174	7.949773	-0.042919	4.169048
208.611130	5946.742539	7.954778	-0.042946	4.171774
208.832660	5954.787969	7.959782	-0.042992	4.174494
209.084769	5962.742442	7.964787	-0.043045	4.177182
209.116415	5970.742748	7.969792	-0.043056	4.179881
209.461050	5978.811165	7.974797	-0.043126	4.182605
209.504429	5986.775234	7.979802	-0.043139	4.185289
209.662865	5994.823264	7.984806	-0.043174	4.188000
209.761836	6002.884995	7.989811	-0.043198	4.190714
209.968292	6010.941129	7.994816	-0.043242	4.193425
210.162761	6018.986223	7.999821	-0.043283	4.196131
210.257355	6026.876080	8.004826	-0.043306	4.198781
210.666723	6034.937882	8.009830	-0.043388	4.201491
210.932282	6042.874536	8.014835	-0.043443	4.204156
210.887961	6050.924728	8.019840	-0.043440	4.206853
211.191915	6058.946957	8.024845	-0.043502	4.209544
211.387203	6066.945127	8.029850	-0.043544	4.212223
211.436190	6075.013615	8.034854	-0.043558	4.214923
211.290991	6083.000697	8.039859	-0.043537	4.217591
211.455200	6090.986288	8.044864	-0.043573	4.220261
211.519392	6099.052020	8.049869	-0.043590	4.222954
211.828463	6106.989315	8.054874	-0.043653	4.225606
212.109268	6115.075854	8.059878	-0.043711	4.228305
212.177443	6123.088630	8.064883	-0.043729	4.230976
212.065040	6131.122074	8.069888	-0.043713	4.233650
212.222633	6139.164017	8.074893	-0.043748	4.236329
212.373577	6147.122112	8.079898	-0.043782	4.238977
212.692227	6155.196974	8.084902	-0.043847	4.241664
212.796397	6163.135567	8.089907	-0.043871	4.244302
212.984124	6171.183100	8.094912	-0.043912	4.246975
213.489403	6179.193033	8.099917	-0.044011	4.249638
213.809550	6187.221814	8.104922	-0.044076	4.252303
214.391400	6195.225943	8.109926	-0.044190	4.254960
214.386325	6203.321158	8.114931	-0.044195	4.257641
214.379853	6211.283737	8.119936	-0.044199	4.260276
214.615445	6219.316493	8.124941	-0.044248	4.262934
214.768783	6227.286646	8.129946	-0.044282	4.265570
215.051479	6235.364257	8.134950	-0.044340	4.268240
215.031126	6243.370839	8.139955	-0.044342	4.270883
215.302536	6251.461837	8.144960	-0.044398	4.273555
215.526053	6259.493900	8.149965	-0.044445	4.276205
215.298908	6267.427972	8.154970	-0.044408	4.278817
215.804377	6275.473256	8.159974	-0.044507	4.281470
215.906602	6283.421048	8.164979	-0.044532	4.284086
215.889860	6291.473606	8.169984	-0.044534	4.286735
216.079564	6299.487974	8.174989	-0.044575	4.289370
216.148704	6307.532216	8.179994	-0.044593	4.292013
216.280113	6315.607509	8.184998	-0.044623	4.294665
216.583274	6323.594175	8.190003	-0.044685	4.297287
216.616119	6331.543818	8.195008	-0.044696	4.299894
216.904148	6339.587487	8.200013	-0.044755	4.302532
217.080260	6347.585476	8.205018	-0.044794	4.305152
217.166249	6355.613450	8.210022	-0.044815	4.307780
217.036023	6363.679130	8.215027	-0.044796	4.310416
217.182995	6371.679242	8.220032	-0.044829	4.313032
217.422936	6379.711773	8.225037	-0.044879	4.315658
217.553238	6387.699191	8.230042	-0.044909	4.318266
217.607863	6395.720973	8.235046	-0.044924	4.320884
217.661979	6403.678699	8.240051	-0.044940	4.323479
217.646393	6411.715626	8.245056	-0.044942	4.326098
218.052291	6419.750992	8.250061	-0.045023	4.328717
218.098105	6427.767615	8.255066	-0.045037	4.331327
218.135013	6435.814256	8.260070	-0.045050	4.333944
218.525085	6443.835132	8.265075	-0.045128	4.336554
218.600094	6451.766781	8.270080	-0.045147	4.339131
218.854151	6459.875430	8.275085	-0.045200	4.341766
218.937039	6467.816559	8.280090	-0.045221	4.344343
219.141576	6475.904383	8.285094	-0.045264	4.346967
219.126940	6483.879301	8.290099	-0.045267	4.349551
219.368846	6491.979096	8.295104	-0.045317	4.352176
219.650386	6500.020377	8.300109	-0.045375	4.354781
219.513233	6507.984196	8.305114	-0.045355	4.357356
219.645337	6515.965716	8.310118	-0.045385	4.359938
219.922257	6523.964658	8.315123	-0.045442	4.362524
220.039608	6531.939641	8.320128	-0.045469	4.365100
220.324704	6540.035201	8.325133	-0.045528	4.367714
220.313302	6548.006768	8.330138	-0.045531	4.370285
220.605971	6556.034485	8.335142	-0.045591	4.372875
220.845399	6564.056442	8.340147	-0.045641	4.375460
221.034127	6572.027920	8.345152	-0.045682	4.378028
221.206816	6580.083069	8.350157	-0.045719	4.380621
221.358127	6588.056048	8.355162	-0.045753	4.383185
221.609610	6596.084456	8.360166	-0.045805	4.385767
221.820179	6604.163150	8.365171	-0.045850	4.388363
221.796372	6612.153511	8.370176	-0.045851	4.390928
221.926044	6620.238379	8.375181	-0.045880	4.393522
221.878058	6628.235654	8.380186	-0.045877	4.396086
222.330427	6636.159968	8.385190	-0.045966	4.398627
222.412798	6644.211255	8.390195	-0.045987	4.401206
222.417740	6652.169051	8.395200	-0.045993	4.403753
222.653896	6660.257558	8.400205	-0.046043	4.406342
222.635485	6668.240713	8.405210	-0.046045	4.408893
222.634569	6676.315211	8.410214	-0.046050	4.411473
222.842353	6684.351074	8.415219	-0.046094	4.414040
223.046498	6692.334024	8.420224	-0.046138	4.416589
223.513973	6700.373467	8.425229	-0.046230	4.419155
223.228365	6708.379162	8.430234	-0.046182	4.421705
223.637618	6716.346682	8.435238	-0.046264	4.424245
223.595916	6724.397181	8.440243	-0.046262	4.426808
223.759598	6732.443471	8.445248	-0.046298	4.429369
223.841906	6740.505476	8.450253	-0.046318	4.431933
223.916576	6748.511375	8.455258	-0.046338	4.434478
224.007059	6756.520708	8.460262	-0.046360	4.437022
223.996149	6764.531154	8.465267	-0.046363	4.439565
224.305115	6772.483797	8.470272	-0.046426	4.442090
224.645672	6780.504690	8.475277	-0.046495	4.444634
224.700679	6788.522248	8.480282	-0.046511	4.447175
224.831827	6796.500051	8.485286	-0.046541	4.449703
225.035966	6804.611749	8.490291	-0.046584	4.452271
225.004133	6812.582120	8.495296	-0.046584	4.454793
225.306588	6820.673374	8.500301	-0.046645	4.457352
225.570219	6828.621636	8.505306	-0.046700	4.459865
225.833115	6836.637787	8.510310	-0.046754	4.462397
225.691987	6844.644560	8.515315	-0.046733	4.464924
225.774995	6852.685896	8.520320	-0.046754	4.467461
226.052119	6860.693975	8.525325	-0.046811	4.469986
226.012742	6868.738984	8.530330	-0.046809	4.472521
226.174855	6876.754600	8.535334	-0.046845	4.475046
226.344725	6884.746949	8.540339	-0.046882	4.477562
226.470155	6892.726470	8.545344	-0.046911	4.480072
226.862935	6900.782243	8.550349	-0.046989	4.482606
227.077002	6908.752127	8.555354	-0.047035	4.485111
227.162583	6916.799450	8.560359	-0.047056	4.487638
227.188218	6924.818107	8.565363	-0.047066	4.490155
227.337494	6932.841087	8.570368	-0.047099	4.492672
227.616442	6940.874383	8.575373	-0.047157	4.495191
227.633752	6948.883822	8.580378	-0.047165	4.497700
227.996889	6956.875672	8.585383	-0.047238	4.500204
227.874725	6964.913339	8.590387	-0.047221	4.502719
227.956485	6972.869828	8.595392	-0.047242	4.505208
228.255852	6980.929812	8.600397	-0.047303	4.507728
228.488922	6988.912020	8.605402	-0.047352	4.510223
228.407465	6996.981293	8.610407	-0.047342	4.512742
228.564583	7005.069183	8.615411	-0.047377	4.515267
228.875443	7012.989279	8.620416	-0.047440	4.517738
229.115340	7021.004533	8.625421	-0.047490	4.520237
229.161010	7028.987652	8.630426	-0.047504	4.522724
229.375311	7036.988035	8.635431	-0.047549	4.525216
229.484860	7045.058867	8.640435	-0.047575	4.527728
229.423531	7053.020922	8.645440	-0.047569	4.530204
229.679781	7061.079678	8.650445	-0.047622	4.532710
229.872692	7069.113248	8.655450	-0.047664	4.535206
230.030569	7077.126401	8.660455	-0.047698	4.537695
229.862379	7085.095645	8.665459	-0.047672	4.540168
230.001674	7093.073452	8.670464	-0.047704	4.542643
230.434546	7101.126575	8.675469	-0.047790	4.545140
230.457383	7109.151220	8.680474	-0.047799	4.547626
230.697000	7117.164030	8.685479	-0.047850	4.550108
230.854958	7125.229146	8.690483	-0.047884	4.552604
230.947223	7133.245565	8.695488	-0.047907	4.555084
231.036111	7141.283583	8.700493	-0.047929	4.557569
231.218224	7149.206364	8.705498	-0.047968	4.560017
231.522930	7157.238137	8.710503	-0.048030	4.562498
231.547130	7165.277549	8.715507	-0.048040	4.564980
231.682532	7173.267279	8.720512	-0.048071	4.567444
232.026020	7181.304192	8.725517	-0.048140	4.569923
231.847372	7189.349411	8.730522	-0.048113	4.572402
232.045712	7197.343985	8.735527	-0.048155	4.574864
232.271448	7205.378378	8.740531	-0.048202	4.577337
232.329606	7213.341553	8.745536	-0.048219	4.579787
232.449436	7221.416519	8.750541	-0.048246	4.582270
232.561704	7229.384156	8.755546	-0.048273	4.584718
232.676143	7237.442523	8.760551	-0.048299	4.587194
232.878541	7245.460355	8.765555	-0.048342	4.589655
232.932611	7253.483869	8.770560	-0.048358	4.592117
233.019554	7261.568695	8.775565	-0.048380	4.594596
233.120826	7269.519331	8.780570	-0.048404	4.597033
233.378261	7277.508699	8.785575	-0.048457	4.599480
233.565970	7285.561668	8.790579	-0.048498	4.601945
233.480202	7293.492720	8.795584	-0.048487	4.604372
233.732227	7301.575768	8.800589	-0.048539	4.606844
233.587700	7309.535743	8.805594	-0.048518	4.609277
233.955613	7317.592752	8.810599	-0.048592	4.611738
234.172233	7325.626616	8.815603	-0.048638	4.614191
234.311712	7333.679167	8.820608	-0.048669	4.616649
234.478020	7341.633690	8.825613	-0.048705	4.619075
234.478507	7349.674340	8.830618	-0.048711	4.621526
234.657884	7357.630218	8.835623	-0.048750	4.623950
234.907775	7365.716548	8.840627	-0.048802	4.626412
234.980277	7373.675765	8.845632	-0.048821	4.628835
234.972450	7381.778703	8.850637	-0.048825	4.631299
235.112829	7389.746488	8.855642	-0.048856	4.633722
235.346641	7397.771072	8.860647	-0.048905	4.636160
235.565049	7405.773217	8.865651	-0.048951	4.638590
235.625114	7413.745376	8.870656	-0.048968	4.641010
235.790586	7421.781665	8.875661	-0.049004	4.643448
235.861836	7429.799363	8.880666	-0.049023	4.645879
235.850717	7437.809745	8.885671	-0.049026	4.648307
236.023063	7445.843394	8.890675	-0.049063	4.650740
236.084869	7453.864488	8.895680	-0.049080	4.653168
236.315274	7461.912020	8.900685	-0.049129	4.655603
236.487423	7469.882089	8.905690	-0.049166	4.658013
236.529146	7477.877585	8.910695	-0.049179	4.660430
236.764541	7485.914171	8.915699	-0.049229	4.662858
236.758437	7493.906506	8.920704	-0.049233	4.665271
237.228822	7501.938094	8.925709	-0.049326	4.667694
237.093776	7509.936190	8.930714	-0.049306	4.670107
237.119053	7518.064449	8.935719	-0.049316	4.672558
237.293925	7526.102361	8.940723	-0.049354	4.674979
237.449701	7534.057321	8.945728	-0.049389	4.677375
237.522841	7542.051273	8.950733	-0.049408	4.679781
237.625679	7550.048497	8.955738	-0.049432	4.682187
238.153898	7558.008626	8.960743	-0.049536	4.684579
238.213343	7566.030608	8.965747	-0.049553	4.686990
238.082200	7574.014034	8.970752	-0.049534	4.689389
238.388253	7582.117564	8.975757	-0.049596	4.691821
238.406556	7590.097681	8.980762	-0.049605	4.694216
238.517344	7598.143923	8.985767	-0.049631	4.696629
238.827596	7606.133189	8.990771	-0.049694	4.699023
238.999761	7614.136126	8.995776	-0.049732	4.701420
239.198519	7622.168439	9.000781	-0.049774	4.703825
239.149271	7630.204180	9.005786	-0.049770	4.706230
239.285781	7638.154594	9.010791	-0.049801	4.708608
239.527811	7646.203899	9.015795	-0.049852	4.711014
239.515543	7654.220930	9.020800	-0.049855	4.713410
239.646981	7662.295481	9.025805	-0.049885	4.715822
239.867362	7670.265126	9.030810	-0.049931	4.718200
239.997367	7678.285215	9.035815	-0.049961	4.720593
240.210214	7686.289208	9.040819	-0.050006	4.722979
240.167303	7694.296119	9.045824	-0.050003	4.725366
240.260561	7702.335557	9.050829	-0.050026	4.727761
240.399695	7710.307178	9.055834	-0.050057	4.730134
240.698588	7718.390349	9.060839	-0.050118	4.732539
240.755551	7726.402986	9.065843	-0.050134	4.734923
240.742741	7734.425306	9.070848	-0.050137	4.737308
241.000144	7742.371365	9.075853	-0.050191	4.739668
241.181864	7750.443731	9.080858	-0.050230	4.742066
241.291377	7758.442717	9.085863	-0.050256	4.744440
241.402461	7766.501557	9.090867	-0.050282	4.746831
241.525847	7774.414066	9.095872	-0.050310	4.749177
241.599621	7782.571252	9.100877	-0.050330	4.751595
241.492561	7790.552470	9.105882	-0.050315	4.753959
241.709875	7798.560307	9.110887	-0.050361	4.756330
242.020985	7806.529003	9.115891	-0.050424	4.758687
241.999098	7814.502077	9.120896	-0.050425	4.761046
242.227905	7822.557095	9.125901	-0.050474	4.763427
242.311348	7830.534160	9.130906	-0.050494	4.765784
242.246860	7838.597963	9.135911	-0.050488	4.768166
242.291013	7846.595220	9.140915	-0.050502	4.770527
242.482251	7854.620563	9.145920	-0.050543	4.772894
242.647341	7862.661281	9.150925	-0.050579	4.775265
242.770043	7870.641949	9.155930	-0.050607	4.777617
242.923457	7878.657751	9.160935	-0.050641	4.779979
243.060464	7886.630704	9.165939	-0.050672	4.782326
243.108636	7894.677496	9.170944	-0.050686	4.784694
243.366965	7902.718492	9.175949	-0.050740	4.787059
243.464873	7910.709268	9.180954	-0.050763	4.789408
243.655780	7918.739345	9.185959	-0.050804	4.791767
243.545527	7926.787163	9.190963	-0.050789	4.794132
243.670714	7934.776442	9.195968	-0.050818	4.796477
243.774985	7942.760863	9.200973	-0.050843	4.798820
243.849476	7950.803078	9.205978	-0.050862	4.801179
244.067226	7958.723660	9.210983	-0.050908	4.803500
244.199667	7966.833332	9.215987	-0.050938	4.805876
244.368574	7974.794118	9.220992	-0.050975	4.808207
244.503965	7982.869244	9.225997	-0.051006	4.810570
244.766962	7990.242887	9.231002	-0.051060	4.812726
244.669914	7994.719893	9.236007	-0.051045	4.814036

244.741028	7997.244787	9.241011	-0.051060	4.814774
244.844730	7998.475399	9.246016	-0.051080	4.815134
244.896252	7998.993044	9.251021	-0.051090	4.815285
244.837195	7999.898658	9.256026	-0.051080	4.815550
245.010765	7999.887620	9.261031	-0.051113	4.815546
245.384973	7999.918291	9.266035	-0.051182	4.815553
245.304482	7999.911658	9.271040	-0.051168	4.815552
245.343970	7999.952897	9.276045	-0.051175	4.815563
245.374475	7999.925647	9.281050	-0.051181	4.815555
245.539281	7999.933687	9.286055	-0.051212	4.815557
245.583337	7999.919472	9.291059	-0.051220	4.815552
245.614958	7999.910394	9.296064	-0.051226	4.815550
245.720978	7999.939902	9.301069	-0.051246	4.815558
245.689363	7999.906301	9.306074	-0.051241	4.815548
245.571942	7999.911881	9.311079	-0.051219	4.815550
245.645096	7999.907750	9.316083	-0.051233	4.815549
245.685103	7999.837941	9.321088	-0.051240	4.815528
245.683447	7999.920155	9.326093	-0.051240	4.815552
245.977133	7999.910007	9.331098	-0.051295	4.815548
246.041608	7999.900396	9.336103	-0.051307	4.815545
246.007629	7999.943642	9.341107	-0.051301	4.815557
246.129419	7999.943507	9.346112	-0.051324	4.815557
246.275497	7999.957651	9.351117	-0.051352	4.815560
246.016659	7999.940637	9.356122	-0.051304	4.815557
245.957200	7999.920464	9.361127	-0.051293	4.815551
246.093724	7999.924841	9.366131	-0.051318	4.815552
246.118156	7999.896424	9.371136	-0.051323	4.815543
246.351840	7999.948302	9.376141	-0.051367	4.815557
246.126736	7999.889123	9.381146	-0.051325	4.815541
246.225940	7999.904639	9.386151	-0.051344	4.815545
246.125671	7999.950008	9.391155	-0.051325	4.815559
246.104150	7999.929385	9.396160	-0.051321	4.815553
246.477654	7999.929081	9.401165	-0.051391	4.815551
246.327394	7999.945871	9.406170	-0.051363	4.815557
246.201063	7999.952373	9.411175	-0.051340	4.815559
246.553962	7999.963480	9.416179	-0.051406	4.815561
246.528136	7999.929972	9.421184	-0.051401	4.815551
246.425592	7999.959287	9.426189	-0.051383	4.815560
246.320484	7999.920216	9.431194	-0.051363	4.815549
246.279460	7999.932379	9.436199	-0.051356	4.815553
246.413290	7999.935645	9.441203	-0.051381	4.815553
246.593645	7999.924719	9.446208	-0.051415	4.815549
246.637361	7999.970299	9.451213	-0.051423	4.815562
246.297058	7999.912445	9.456218	-0.051360	4.815547
246.335303	7999.934443	9.461223	-0.051367	4.815553
246.545515	7999.948564	9.466227	-0.051406	4.815556
246.317817	7999.904292	9.471232	-0.051364	4.815544
246.513617	7999.941671	9.476237	-0.051401	4.815554
246.510040	7999.921341	9.481242	-0.051400	4.815548
246.752321	7999.897542	9.486247	-0.051446	4.815540
246.800079	7999.941052	9.491251	-0.051455	4.815553
246.572167	7999.897844	9.496256	-0.051413	4.815541
246.808359	7999.989276	9.501261	-0.051457	4.815567
246.705485	7999.940630	9.506266	-0.051438	4.815553
246.480976	7999.935920	9.511271	-0.051396	4.815553
246.658090	7999.930281	9.516275	-0.051429	4.815550
246.652028	7999.953692	9.521280	-0.051428	4.815557
246.652827	7999.970809	9.526285	-0.051429	4.815562
246.535193	7999.925126	9.531290	-0.051407	4.815549
246.792065	7999.856714	9.536295	-0.051455	4.815528
246.623283	7999.910578	9.541299	-0.051424	4.815545
246.637498	7999.919370	9.546304	-0.051427	4.815547
246.670844	7999.948763	9.551309	-0.051433	4.815556
246.697585	7999.926790	9.556314	-0.051438	4.815549
246.706291	7999.915203	9.561319	-0.051440	4.815546
246.896825	7999.952497	9.566323	-0.051476	4.815556
246.845858	7999.923919	9.571328	-0.051466	4.815547
246.843416	7999.991173	9.576333	-0.051466	4.815567
246.964196	7999.965394	9.581338	-0.051489	4.815559
247.052985	7999.955111	9.586343	-0.051506	4.815556
247.038185	7999.967702	9.591347	-0.051503	4.815559
246.896147	7999.903467	9.596352	-0.051477	4.815541
247.079612	7999.962004	9.601357	-0.051511	4.815557
246.945897	7999.967317	9.606362	-0.051486	4.815560
247.002719	7999.951174	9.611367	-0.051497	4.815555
246.869363	7999.951154	9.616371	-0.051473	4.815555
247.158405	7999.935592	9.621376	-0.051527	4.815549
247.050992	7999.971235	9.626381	-0.051507	4.815560
246.896439	7999.949511	9.631386	-0.051478	4.815555
246.900213	7999.947454	9.636391	-0.051479	4.815554
246.997082	7999.941575	9.641395	-0.051497	4.815552
247.023658	7999.921735	9.646400	-0.051503	4.815546
247.191888	7999.969346	9.651405	-0.051534	4.815559
247.173158	7999.959447	9.656410	-0.051531	4.815556
247.330928	7999.964172	9.661415	-0.051560	4.815557
247.249000	7999.956446	9.666419	-0.051545	4.815555
247.267766	7999.937547	9.671424	-0.051549	4.815549
247.309910	7999.990578	9.676429	-0.051557	4.815565
247.049616	7999.955383	9.681434	-0.051509	4.815556
247.108900	7999.969181	9.686439	-0.051520	4.815559
247.190235	7999.985475	9.691443	-0.051535	4.815564
246.966946	7999.969037	9.696448	-0.051494	4.815560
247.088669	7999.980650	9.701453	-0.051517	4.815563
247.322686	7999.937495	9.706458	-0.051561	4.815549
247.184764	7999.969436	9.711463	-0.051535	4.815559
247.197063	7999.994215	9.716467	-0.051538	4.815566
247.259372	7999.982433	9.721472	-0.051549	4.815562
247.103696	7999.974573	9.726477	-0.051521	4.815561
247.158377	7999.941309	9.731482	-0.051531	4.815551
247.286470	7999.974384	9.736487	-0.051555	4.815560
247.421987	7999.989425	9.741491	-0.051580	4.815564
247.358790	7999.952103	9.746496	-0.051569	4.815553
247.453631	7999.964346	9.751501	-0.051587	4.815556
247.451185	7999.950440	9.756506	-0.051586	4.815552
247.423077	7999.947863	9.761511	-0.051581	4.815552
247.149276	7999.969046	9.766515	-0.051531	4.815559
247.198056	7999.952773	9.771520	-0.051540	4.815554
247.239605	7999.973757	9.776525	-0.051548	4.815560
247.189248	7999.943052	9.781530	-0.051539	4.815551
247.522608	7999.922875	9.786535	-0.051601	4.815544
247.404270	7999.950864	9.791539	-0.051579	4.815552
247.273310	7999.932727	9.796544	-0.051555	4.815548
247.177337	7999.985643	9.801549	-0.051537	4.815564
247.383571	7999.931356	9.806554	-0.051576	4.815547
247.243261	7999.926950	9.811559	-0.051550	4.815546
247.145859	7999.969163	9.816563	-0.051532	4.815559
247.258787	7999.911219	9.821568	-0.051553	4.815542
247.313147	7999.999689	9.826573	-0.051564	4.815567
247.275009	7999.973455	9.831578	-0.051557	4.815560
247.279340	7999.976747	9.836583	-0.051558	4.815561
247.559210	7999.954629	9.841587	-0.051610	4.815553
247.476062	7999.928729	9.846592	-0.051595	4.815546
247.456988	7999.957269	9.851597	-0.051591	4.815554
247.554733	7999.955676	9.856602	-0.051610	4.815553
247.442776	7999.942121	9.861607	-0.051589	4.815550
247.388408	7999.964745	9.866611	-0.051579	4.815557
247.445110	7999.937922	9.871616	-0.051590	4.815548
247.580167	7999.979653	9.876621	-0.051615	4.815560
247.312332	7999.965693	9.881626	-0.051566	4.815557
247.256901	7999.992571	9.886631	-0.051555	4.815565
247.460578	7999.987366	9.891635	-0.051594	4.815563
247.499676	7999.990156	9.896640	-0.051601	4.815563
247.391616	8000.001226	9.901645	-0.051581	4.815567
247.464141	7999.982136	9.906650	-0.051595	4.815561
247.526296	7999.991710	9.911655	-0.051607	4.815564
247.676633	7999.986703	9.916659	-0.051635	4.815562
247.625779	7999.985891	9.921664	-0.051625	4.815562
247.656329	7999.998153	9.926669	-0.051631	4.815565
247.444278	7999.951997	9.931674	-0.051592	4.815552
247.567797	7999.951892	9.936679	-0.051615	4.815552
247.446817	7999.986246	9.941683	-0.051593	4.815562
247.535521	7999.955672	9.946688	-0.051610	4.815553
247.605573	7999.992072	9.951693	-0.051623	4.815563
247.416163	7999.996476	9.956698	-0.051588	4.815566
247.782123	7999.988578	9.961703	-0.051656	4.815562
247.662569	8000.012275	9.966707	-0.051634	4.815569
247.682337	7999.968831	9.971712	-0.051638	4.815556
247.903897	8000.019449	9.976717	-0.051679	4.815570
247.768284	7999.990557	9.981722	-0.051654	4.815562
247.743776	7999.977359	9.986727	-0.051650	4.815558
247.815100	8000.002034	9.991731	-0.051663	4.815565
247.700838	7999.980965	9.996736	-0.051642	4.815560
247.557449	8000.010681	10.001741	-0.051616	4.815569
247.706450	7999.975752	10.006746	-0.051644	4.815558
247.720208	7999.980265	10.011751	-0.051647	4.815559
247.649253	7999.973785	10.016755	-0.051634	4.815558
247.595727	7999.965455	10.021760	-0.051624	4.815556
247.594542	7999.980403	10.026765	-0.051624	4.815560
247.685401	7999.985105	10.031770	-0.051641	4.815561
247.512701	7999.975899	10.036775	-0.051609	4.815559
247.811773	7999.976521	10.041779	-0.051665	4.815558
247.726357	7999.932430	10.046784	-0.051649	4.815545
247.641278	7999.979115	10.051789	-0.051633	4.815559
247.666874	7999.977414	10.056794	-0.051638	4.815559
247.583468	7999.957917	10.061799	-0.051623	4.815553
247.773991	7999.968516	10.066803	-0.051659	4.815556
247.534778	7999.943275	10.071808	-0.051614	4.815549
247.599148	7999.985990	10.076813	-0.051627	4.815562
247.757775	7999.977914	10.081818	-0.051656	4.815558
247.795129	7999.947571	10.086823	-0.051663	4.815549
247.825036	8000.001471	10.091827	-0.051669	4.815565
247.800943	7999.959447	10.096832	-0.051665	4.815553
247.734011	7999.986139	10.101837	-0.051653	4.815561
247.754940	7999.955528	10.106842	-0.051657	4.815552
247.821709	7999.934208	10.111847	-0.051669	4.815545
247.842589	7999.992232	10.116851	-0.051673	4.815562
247.710494	7999.923886	10.121856	-0.051649	4.815543
247.792338	7999.944460	10.126861	-0.051665	4.815548
247.884478	7999.972677	10.131866	-0.051682	4.815556
247.720906	7999.960416	10.136871	-0.051652	4.815553
247.742220	7999.984274	10.141875	-0.051656	4.815560
247.935946	7999.955413	10.146880	-0.051692	4.815551
247.932202	7999.990610	10.151885	-0.051692	4.815561
247.882694	7999.964190	10.156890	-0.051683	4.815554
247.926717	7999.959586	10.161895	-0.051691	4.815552
247.791610	7999.980894	10.166899	-0.051666	4.815559
247.840704	7999.942199	10.171904	-0.051675	4.815547
247.831446	7999.958084	10.176909	-0.051674	4.815552
247.961466	7999.971968	10.181914	-0.051698	4.815556
247.753517	7999.944033	10.186919	-0.051660	4.815548
247.898967	7999.995546	10.191923	-0.051687	4.815563
247.744335	7999.921492	10.196928	-0.051658	4.815542
247.805951	7999.965230	10.201933	-0.051670	4.815554
247.919755	7999.971374	10.206938	-0.051691	4.815556
248.011120	7999.958998	10.211943	-0.051709	4.815552
248.073118	8000.020898	10.216947	-0.051720	4.815569
247.827893	7999.938959	10.221952	-0.051675	4.815547
247.972209	7999.932786	10.226957	-0.051702	4.815544
248.016850	7999.938870	10.231962	-0.051710	4.815546
247.966718	7999.963700	10.236967	-0.051701	4.815553
248.103058	7999.990503	10.241971	-0.051727	4.815560
248.076208	7999.972995	10.246976	-0.051722	4.815555
247.986646	7999.990774	10.251981	-0.051706	4.815561
248.060155	8000.004805	10.256986	-0.051720	4.815565
248.247108	7999.980106	10.261991	-0.051755	4.815557
248.208776	8000.024350	10.266995	-0.051748	4.815570
247.890841	7999.975398	10.272000	-0.051689	4.815557
247.966925	7999.979859	10.277005	-0.051703	4.815558
248.117696	7999.978064	10.282010	-0.051731	4.815557
248.133801	7999.970868	10.287015	-0.051734	4.815554
248.144057	8000.025517	10.292019	-0.051737	4.815570
248.029847	7999.982022	10.297024	-0.051715	4.815558
248.292538	7999.964965	10.302029	-0.051765	4.815552
248.200465	7999.989111	10.307034	-0.051748	4.815559
248.138840	7999.981716	10.312039	-0.051736	4.815557
248.070595	8000.009454	10.317043	-0.051724	4.815566
248.015788	7999.985083	10.322048	-0.051714	4.815559
248.152507	7999.971311	10.327053	-0.051739	4.815554
248.209980	7999.978673	10.332058	-0.051750	4.815556
247.997630	7999.950665	10.337063	-0.051711	4.815549
248.257242	8000.005108	10.342067	-0.051760	4.815564
248.259106	7999.964575	10.347072	-0.051760	4.815552
248.103408	8000.000498	10.352077	-0.051731	4.815563
248.045649	7999.996369	10.357082	-0.051721	4.815562
248.166818	7999.979140	10.362087	-0.051743	4.815557
248.334038	8000.031009	10.367091	-0.051775	4.815571
248.093286	7999.973704	10.372096	-0.051730	4.815555
247.932689	8000.002071	10.377101	-0.051700	4.815564
248.170868	7999.967528	10.382106	-0.051745	4.815553
248.068791	7999.960541	10.387111	-0.051726	4.815552
247.992668	7999.971064	10.392115	-0.051712	4.815555
248.127759	7999.935907	10.397120	-0.051738	4.815544
248.117641	7999.965661	10.402125	-0.051736	4.815553
248.074870	7999.990610	10.407130	-0.051728	4.815560
248.043468	7999.963417	10.412135	-0.051722	4.815552
248.260320	8000.011824	10.417139	-0.051763	4.815566
248.205490	7999.971434	10.422144	-0.051753	4.815554
248.370622	7999.991231	10.427149	-0.051784	4.815559
248.214778	8000.008997	10.432154	-0.051755	4.815565
248.203525	7999.973589	10.437159	-0.051753	4.815555
248.016781	8000.017549	10.442163	-0.051719	4.815568
248.134211	7999.968221	10.447168	-0.051741	4.815553
248.326152	7999.985252	10.452173	-0.051777	4.815557
248.178523	8000.006356	10.457178	-0.051749	4.815564
248.199149	7999.987487	10.462183	-0.051753	4.815559
248.375739	8000.026694	10.467187	-0.051787	4.815569
248.255437	7999.994847	10.472192	-0.051764	4.815561
248.055137	7999.989461	10.477197	-0.051727	4.815560
248.147216	7999.982437	10.482202	-0.051745	4.815557
248.158482	7999.980502	10.487207	-0.051747	4.815557
248.238982	8000.003190	10.492211	-0.051762	4.815563
248.072397	7999.990879	10.497216	-0.051731	4.815560
248.155461	8000.029628	10.502221	-0.051747	4.815571
248.116545	8000.001245	10.507226	-0.051740	4.815563
248.140733	7999.997385	10.512231	-0.051745	4.815562
248.239017	8000.028907	10.517235	-0.051763	4.815571
248.190105	7999.974730	10.522240	-0.051754	4.815555
247.970087	7999.981839	10.527245	-0.051713	4.815558
248.086791	7999.967740	10.532250	-0.051735	4.815553
248.078532	7999.975098	10.537255	-0.051734	4.815556
248.127376	8000.007950	10.542259	-0.051743	4.815565
248.187573	7999.977979	10.547264	-0.051755	4.815556
248.327570	7999.985619	10.552269	-0.051781	4.815557
248.270301	7999.983634	10.557274	-0.051770	4.815557
247.977878	7999.951117	10.562279	-0.051716	4.815549
248.139237	8000.015704	10.567283	-0.051746	4.815567
248.233989	8000.008724	10.572288	-0.051764	4.815565
248.213990	7999.987056	10.577293	-0.051761	4.815558
248.364960	8000.003419	10.582298	-0.051789	4.815562
248.415992	7999.979706	10.587303	-0.051799	4.815555
248.536997	7999.994512	10.592307	-0.051821	4.815559
248.325922	7999.991087	10.597312	-0.051782	4.815559
248.419458	8000.009716	10.602317	-0.051800	4.815564
248.569503	8000.020725	10.607322	-0.051828	4.815567
248.320406	7999.997456	10.612327	-0.051782	4.815561
248.578034	8000.034781	10.617331	-0.051830	4.815571
248.468199	7999.976406	10.622336	-0.051810	4.815554
248.323938	7999.978342	10.627341	-0.051783	4.815555
248.209934	7999.965821	10.632346	-0.051762	4.815552
248.509979	7999.995294	10.637351	-0.051818	4.815559
248.388337	8000.016822	10.642355	-0.051796	4.815566
248.317397	8000.013546	10.647360	-0.051783	4.815566
248.435546	8000.065683	10.652365	-0.051805	4.815580
248.407749	8000.079130	10.657370	-0.051800	4.815584
248.256983	8000.023291	10.662375	-0.051772	4.815569
248.535303	8000.032120	10.667379	-0.051824	4.815570
248.522371	8000.027655	10.672384	-0.051822	4.815569
248.399587	8000.001107	10.677389	-0.051799	4.815562
248.466008	8000.011819	10.682394	-0.051812	4.815564
248.401348	7999.980879	10.687399	-0.051800	4.815556
248.607743	8000.030184	10.692403	-0.051839	4.815569
248.318482	8000.007328	10.697408	-0.051785	4.815564
248.261561	8000.003213	10.702413	-0.051774	4.815563
248.300652	8000.008139	10.707418	-0.051782	4.815564
248.293426	8000.004835	10.712423	-0.051781	4.815563
248.413851	8000.020700	10.717427	-0.051803	4.815567
248.459116	7999.990485	10.722432	-0.051812	4.815558
248.463275	7999.975619	10.727437	-0.051813	4.815554
248.298345	7999.984694	10.732442	-0.051783	4.815557
248.203420	7999.985298	10.737447	-0.051765	4.815558
248.498708	8000.033917	10.742451	-0.051820	4.815571
248.517080	7999.992585	10.747456	-0.051824	4.815558
248.465425	7999.996031	10.752461	-0.051814	4.815560
248.601496	8000.017491	10.757466	-0.051840	4.815565
248.468575	8000.013204	10.762471	-0.051815	4.815565
248.552653	8000.046630	10.767475	-0.051831	4.815574
248.527703	7999.994980	10.772480	-0.051827	4.815559
248.421255	8000.016755	10.777485	-0.051807	4.815566
248.523944	8000.032331	10.782490	-0.051827	4.815570
248.485515	8000.014634	10.787495	-0.051820	4.815565
248.638921	8000.031037	10.792499	-0.051848	4.815569
248.482324	7999.979375	10.797504	-0.051819	4.815555
248.486678	7999.998686	10.802509	-0.051820	4.815560
248.714809	8000.043006	10.807514	-0.051863	4.815572
248.444496	8000.003372	10.812519	-0.051813	4.815562
248.433607	8000.028841	10.817523	-0.051811	4.815569
248.576451	8000.008762	10.822528	-0.051838	4.815563
248.365104	7999.978634	10.827533	-0.051799	4.815555
248.710140	7999.998162	10.832538	-0.051863	4.815559
248.475058	8000.005024	10.837543	-0.051820	4.815562
248.357578	8000.050114	10.842547	-0.051798	4.815576
248.376609	8000.022675	10.847552	-0.051802	4.815568
248.330623	8000.008059	10.852557	-0.051793	4.815564
248.513291	8000.017464	10.857562	-0.051827	4.815566
248.460393	7999.971765	10.862567	-0.051818	4.815552
248.528121	8000.013468	10.867571	-0.051831	4.815564
248.473745	8000.000851	10.872576	-0.051821	4.815561
248.375242	8000.005669	10.877581	-0.051803	4.815563
248.263218	8000.026285	10.882586	-0.051782	4.815569
248.381689	7999.994062	10.887591	-0.051804	4.815559
248.744291	8000.024556	10.892595	-0.051872	4.815567
248.559268	8000.010876	10.897600	-0.051838	4.815563
248.373204	8000.009994	10.902605	-0.051803	4.815564
248.547512	8000.027805	10.907610	-0.051836	4.815568
248.526525	8000.003986	10.912615	-0.051832	4.815562
248.561769	8000.045159	10.917619	-0.051839	4.815573
248.765356	7999.990829	10.922624	-0.051877	4.815557
248.781439	8000.027419	10.927629	-0.051880	4.815567
248.452868	8000.023144	10.932634	-0.051819	4.815567
248.351169	7999.960630	10.937639	-0.051800	4.815550
248.529750	7999.992394	10.942643	-0.051834	4.815558
248.463545	7999.983856	10.947648	-0.051822	4.815556
248.483149	8000.032250	10.952653	-0.051826	4.815570
248.656674	8000.019079	10.957658	-0.051858	4.815565
248.474401	7999.960590	10.962663	-0.051824	4.815549
248.574859	8000.007099	10.967667	-0.051843	4.815562
248.613003	7999.990652	10.972672	-0.051851	4.815557
248.773280	8000.027458	10.977677	-0.051881	4.815567
248.526343	8000.030922	10.982682	-0.051835	4.815569
248.351996	7999.990717	10.987687	-0.051803	4.815558
248.465160	8000.007531	10.992691	-0.051824	4.815563
248.271922	7999.983038	10.997696	-0.051788	4.815557
248.302304	7999.976075	11.002701	-0.051794	4.815554
248.525412	8000.003226	11.007706	-0.051836	4.815561
248.515515	7999.977452	11.012711	-0.051834	4.815554
248.441622	8000.031796	11.017715	-0.051820	4.815570
248.614837	8000.017552	11.022720	-0.051853	4.815565
248.591467	8000.031071	11.027725	-0.051849	4.815569
248.471946	8000.022731	11.032730	-0.051827	4.815567
248.634330	8000.011514	11.037735	-0.051857	4.815563
248.609452	8000.021805	11.042739	-0.051853	4.815566
248.582747	7999.977601	11.047744	-0.051848	4.815553
248.532024	7999.984266	11.052749	-0.051839	4.815556
248.504346	8000.015870	11.057754	-0.051834	4.815565
248.691542	8000.003990	11.062759	-0.051869	4.815561
248.632511	8000.004112	11.067763	-0.051858	4.815561
248.626397	7999.990146	11.072768	-0.051857	4.815557
248.699113	7999.998825	11.077773	-0.051871	4.815559
248.574178	8000.033114	11.082778	-0.051848	4.815570
248.629810	8000.020156	11.087783	-0.051858	4.815566
248.861870	8000.042114	11.092787	-0.051902	4.815571
248.820274	7999.985920	11.097792	-0.051894	4.815555
248.635943	7999.998949	11.102797	-0.051860	4.815559
248.624417	7999.996642	11.107802	-0.051858	4.815559
248.568698	7999.941286	11.112807	-0.051848	4.815543
248.707359	8000.023660	11.117811	-0.051874	4.815566
248.708359	8000.005539	11.122816	-0.051874	4.815561
248.746522	8000.028605	11.127821	-0.051881	4.815567
248.669826	8000.030575	11.132826	-0.051867	4.815568
248.503050	7999.983018	11.137831	-0.051837	4.815555
248.698038	8000.020390	11.142835	-0.051873	4.815565
248.587698	8000.008996	11.147840	-0.051853	4.815562
248.494667	7999.992544	11.152845	-0.051836	4.815558
248.844523	8000.027103	11.157850	-0.051901	4.815567
248.774249	7999.998208	11.162855	-0.051888	4.815558
248.841782	8000.035637	11.167859	-0.051901	4.815569
248.685055	7999.998923	11.172864	-0.051872	4.815559
248.729767	8000.022096	11.177869	-0.051880	4.815566
248.990535	8000.038115	11.182874	-0.051929	4.815569
248.679141	7999.968976	11.187879	-0.051871	4.815550
248.785015	8000.025185	11.192883	-0.051891	4.815566
248.744318	7999.996772	11.197888	-0.051884	4.815558
248.822105	7999.993786	11.202893	-0.051898	4.815557
248.632815	8000.001395	11.207898	-0.051863	4.815560
248.624886	7999.997011	11.212903	-0.051862	4.815559
248.475767	8000.009546	11.217907	-0.051835	4.815563
248.480963	7999.997901	11.222912	-0.051836	4.815560
248.693244	8000.012061	11.227917	-0.051875	4.815563
248.819585	8000.014139	11.232922	-0.051899	4.815563
248.684897	7999.990600	11.237927	-0.051874	4.815557
248.820183	8000.041950	11.242931	-0.051900	4.815571
248.993476	8000.027708	11.247936	-0.051932	4.815566
248.855539	8000.041493	11.252941	-0.051907	4.815571
248.884488	8000.054798	11.257946	-0.051912	4.815574
248.817111	7999.991775	11.262951	-0.051900	4.815556
248.611710	8000.006596	11.267955	-0.051862	4.815562
248.822139	8000.003639	11.272960	-0.051901	4.815560
248.879129	8000.014198	11.277965	-0.051912	4.815562
248.914257	8000.021196	11.282970	-0.051919	4.815564
248.901882	8000.007128	11.287975	-0.051917	4.815560
249.001427	8000.037604	11.292979	-0.051935	4.815569
248.832174	8000.039131	11.297984	-0.051904	4.815570
248.671989	8000.054690	11.302989	-0.051874	4.815575
248.816515	8000.070948	11.307994	-0.051902	4.815579
248.925689	8000.022553	11.312999	-0.051922	4.815565
248.903554	8000.049976	11.318003	-0.051918	4.815573
248.678816	7999.983318	11.323008	-0.051877	4.815554
248.671126	8000.015248	11.328013	-0.051875	4.815564
248.915125	8000.032061	11.333018	-0.051921	4.815567
248.686768	8000.026217	11.338023	-0.051879	4.815567
248.807634	8000.058108	11.343027	-0.051901	4.815576
248.995799	8000.031293	11.348032	-0.051937	4.815567
248.934208	8000.014286	11.353037	-0.051925	4.815562
248.833011	8000.047895	11.358042	-0.051907	4.815572
248.829026	7999.972023	11.363047	-0.051906	4.815550
249.240606	8000.028949	11.368051	-0.051983	4.815565
248.858167	7999.981076	11.373056	-0.051912	4.815553
248.889379	7999.983739	11.378061	-0.051918	4.815553
249.076419	8000.024186	11.383066	-0.051953	4.815564
248.923194	7999.997140	11.388071	-0.051925	4.815557
248.928270	8000.064521	11.393075	-0.051926	4.815577
248.958675	8000.028724	11.398080	-0.051932	4.815566
248.930851	8000.027219	11.403085	-0.051927	4.815566
249.022780	8000.010581	11.408090	-0.051944	4.815561
248.965014	8000.016063	11.413095	-0.051933	4.815562
249.130448	8000.039071	11.418099	-0.051964	4.815568
249.002208	8000.022044	11.423104	-0.051941	4.815564
248.899177	8000.048147	11.428109	-0.051922	4.815572
249.089985	8000.067297	11.433114	-0.051957	4.815577
248.935889	8000.049848	11.438119	-0.051929	4.815572
248.881438	8000.058589	11.443123	-0.051919	4.815575
248.960579	8000.027859	11.448128	-0.051934	4.815566
248.881676	8000.024453	11.453133	-0.051919	4.815565
248.762840	8000.030007	11.458138	-0.051897	4.815567
248.616094	8000.008407	11.463143	-0.051870	4.815562
248.959862	8000.046071	11.468147	-0.051935	4.815571
248.713605	7999.982266	11.473152	-0.051889	4.815554
248.829561	7999.987378	11.478157	-0.051911	4.815555
248.951856	8000.015022	11.483162	-0.051934	4.815562
248.972953	7999.996160	11.488167	-0.051938	4.815557
249.055437	8000.058396	11.493171	-0.051953	4.815574
249.019492	8000.034332	11.498176	-0.051947	4.815567
249.137866	8000.037349	11.503181	-0.051969	4.815568
249.139345	8000.039526	11.508186	-0.051970	4.815568
248.986203	7999.996462	11.513191	-0.051941	4.815557
249.054241	8000.046715	11.518195	-0.051954	4.815571
249.061869	8000.036177	11.523200	-0.051956	4.815568
248.939576	8000.034199	11.528205	-0.051933	4.815568
248.939225	8000.042754	11.533210	-0.051933	4.815570
248.784946	8000.032778	11.538215	-0.051905	4.815568
248.918891	8000.040321	11.543219	-0.051930	4.815570
248.898043	7999.991940	11.548224	-0.051926	4.815556
248.730954	8000.004183	11.553229	-0.051895	4.815560
248.948467	8000.035515	11.558234	-0.051936	4.815568
248.830455	8000.015452	11.563239	-0.051914	4.815563
248.832414	8000.022977	11.568243	-0.051915	4.815565
248.831554	8000.012300	11.573248	-0.051915	4.815562
248.750371	8000.008857	11.578253	-0.051900	4.815561
248.843506	8000.044568	11.583258	-0.051917	4.815571
248.820682	8000.029262	11.588263	-0.051913	4.815567
248.815294	8000.069773	11.593267	-0.051913	4.815579
248.904997	8000.038147	11.598272	-0.051929	4.815569
248.790192	8000.022408	11.603277	-0.051908	4.815565
248.827363	8000.014488	11.608282	-0.051915	4.815562
248.721480	8000.024525	11.613287	-0.051896	4.815566
248.884351	8000.023996	11.618291	-0.051926	4.815565
248.956105	8000.067902	11.623296	-0.051940	4.815577
248.868043	8000.031240	11.628301	-0.051924	4.815567
248.805539	8000.035577	11.633306	-0.051912	4.815569
248.816243	8000.014410	11.638311	-0.051914	4.815562
248.823643	8000.024160	11.643315	-0.051916	4.815565
248.770723	8000.007294	11.648320	-0.051906	4.815561
248.927677	8000.050454	11.653325	-0.051936	4.815572
248.874502	8000.061351	11.658330	-0.051926	4.815576
248.710196	7999.996747	11.663335	-0.051896	4.815558
249.117068	8000.036509	11.668339	-0.051972	4.815567
249.250999	8000.025897	11.673344	-0.051997	4.815564
248.995730	8000.029224	11.678349	-0.051949	4.815566
248.918694	8000.023712	11.683354	-0.051935	4.815565
249.068926	8000.011230	11.688359	-0.051963	4.815560
248.960776	8000.025501	11.693363	-0.051944	4.815565
248.995940	8000.006869	11.698368	-0.051950	4.815559
249.204641	8000.033787	11.703373	-0.051989	4.815566
249.027746	8000.062956	11.708378	-0.051957	4.815576
248.989642	7999.989731	11.713383	-0.051950	4.815554
249.059136	8000.043212	11.718387	-0.051963	4.815570
248.924620	8000.030354	11.723392	-0.051938	4.815567
248.840907	8000.023666	11.728397	-0.051923	4.815565
248.980631	8000.049458	11.733402	-0.051949	4.815572
248.978405	7999.987498	11.738407	-0.051949	4.815554
249.147102	8000.021238	11.743411	-0.051980	4.815563
249.090084	8000.014985	11.748416	-0.051970	4.815561
249.002348	7999.997551	11.753421	-0.051954	4.815557
249.181764	8000.052826	11.758426	-0.051987	4.815572
249.020232	8000.019237	11.763431	-0.051957	4.815563
249.186942	8000.029450	11.768435	-0.051989	4.815565
249.260777	8000.017857	11.773440	-0.052003	4.815561
249.096966	8000.021608	11.778445	-0.051972	4.815563
249.180898	8000.021927	11.783450	-0.051988	4.815563
249.460969	8000.001952	11.788455	-0.052040	4.815556
249.330589	8000.027608	11.793459	-0.052016	4.815564
249.211735	8000.045977	11.798464	-0.051994	4.815570
249.269066	8000.019163	11.803469	-0.052005	4.815562
249.353271	8000.046186	11.808474	-0.052021	4.815569
249.226592	8000.024912	11.813479	-0.051998	4.815563
249.321759	8000.056385	11.818483	-0.052016	4.815572
249.141929	8000.010749	11.823488	-0.051982	4.815560
249.026492	7999.996068	11.828493	-0.051961	4.815556
249.365821	8000.044341	11.833498	-0.052024	4.815568
249.281727	8000.012015	11.838503	-0.052009	4.815559
249.403940	8000.055677	11.843507	-0.052032	4.815572
249.291295	8000.059195	11.848512	-0.052011	4.815573
249.116458	8000.054223	11.853517	-0.051979	4.815572
249.359289	8000.052864	11.858522	-0.052024	4.815571
249.083433	8000.017408	11.863527	-0.051973	4.815562
249.121697	8000.034069	11.868531	-0.051980	4.815567
249.178156	8000.016852	11.873536	-0.051991	4.815561
249.029849	8000.014449	11.878541	-0.051964	4.815561
249.102528	8000.041284	11.883546	-0.051977	4.815569
249.137419	8000.010900	11.888551	-0.051984	4.815560
249.136096	8000.027982	11.893555	-0.051984	4.815565
248.974709	8000.020026	11.898560	-0.051954	4.815563
249.005028	8000.008791	11.903565	-0.051960	4.815560
249.300776	8000.038197	11.908570	-0.052015	4.815567
249.119794	7999.992543	11.913575	-0.051982	4.815554
249.230552	8000.038154	11.918579	-0.052003	4.815567
249.302579	8000.026531	11.923584	-0.052016	4.815563
249.270152	8000.007864	11.928589	-0.052010	4.815558
249.262381	8000.025909	11.933594	-0.052009	4.815563
249.266341	8000.015311	11.938599	-0.052010	4.815560
249.435365	8000.060806	11.943603	-0.052042	4.815573
249.283622	8000.029511	11.948608	-0.052014	4.815564
249.207218	8000.000515	11.953613	-0.052000	4.815556
249.251668	8000.038636	11.958618	-0.052008	4.815567
249.219926	8000.026387	11.963623	-0.052002	4.815564
249.271254	8000.037922	11.968627	-0.052012	4.815567
249.324925	8000.053766	11.973632	-0.052022	4.815571
249.078115	8000.020921	11.978637	-0.051977	4.815563
249.155932	8000.039295	11.983642	-0.051991	4.815568
249.082701	8000.016758	11.988647	-0.051978	4.815562
249.305050	8000.043899	11.993651	-0.052019	4.815568
249.233489	8000.045952	11.998656	-0.052006	4.815569
249.308667	8000.032245	12.003661	-0.052021	4.815565
249.374408	8000.042947	12.008666	-0.052033	4.815568
249.276002	8000.027475	12.013671	-0.052015	4.815564
249.178349	8000.059005	12.018675	-0.051997	4.815573
249.284290	8000.051139	12.023680	-0.052017	4.815571
249.235239	8000.036473	12.028685	-0.052008	4.815567
249.144087	8000.059565	12.033690	-0.051991	4.815574
249.069517	8000.008172	12.038695	-0.051977	4.815559
249.213948	8000.036177	12.043699	-0.052004	4.815567
249.271051	8000.029650	12.048704	-0.052015	4.815564
249.284143	8000.007454	12.053709	-0.052018	4.815558
249.498393	8000.050483	12.058714	-0.052058	4.815569
249.185862	8000.014428	12.063719	-0.052000	4.815560
249.254641	8000.040131	12.068723	-0.052013	4.815567
249.311542	8000.053892	12.073728	-0.052024	4.815571
249.288224	8000.015082	12.078733	-0.052020	4.815560
249.291365	8000.036510	12.083738	-0.052020	4.815566
249.220466	8000.014011	12.088743	-0.052007	4.815560
249.518823	8000.054140	12.093747	-0.052063	4.815570
249.469406	8000.031992	12.098752	-0.052054	4.815564
249.147280	8000.035295	12.103757	-0.051994	4.815567
249.301719	8000.055988	12.108762	-0.052023	4.815572
249.400362	8000.014897	12.113767	-0.052042	4.815559
249.129682	8000.035060	12.118771	-0.051992	4.815567
249.291932	8000.017434	12.123776	-0.052022	4.815561
249.539852	8000.014021	12.128781	-0.052068	4.815558
249.484941	8000.064405	12.133786	-0.052058	4.815573
249.368160	8000.021933	12.138791	-0.052037	4.815562
249.337874	8000.057767	12.143795	-0.052031	4.815572
249.403674	8000.051382	12.148800	-0.052044	4.815570
249.425400	8000.054958	12.153805	-0.052048	4.815571
249.537112	8000.074954	12.158810	-0.052069	4.815576
249.575181	8000.027534	12.163815	-0.052076	4.815562
249.447536	8000.050031	12.168819	-0.052053	4.815569
249.446818	8000.021202	12.173824	-0.052053	4.815561
249.253015	7999.993493	12.178829	-0.052017	4.815554
249.150175	8000.047365	12.183834	-0.051998	4.815570
249.235256	7999.996441	12.188839	-0.052014	4.815555
249.353753	8000.046450	12.193843	-0.052036	4.815569
249.402675	8000.034451	12.198848	-0.052046	4.815565
249.385423	8000.036322	12.203853	-0.052043	4.815566
249.509107	8000.063989	12.208858	-0.052066	4.815573
249.451415	8000.018210	12.213863	-0.052055	4.815560
249.224305	8000.038016	12.218867	-0.052013	4.815567
249.287553	8000.042269	12.223872	-0.052025	4.815568
249.499846	8000.045751	12.228877	-0.052065	4.815568
249.416148	8000.042267	12.233882	-0.052050	4.815567
249.416197	8000.033741	12.238887	-0.052050	4.815565
249.597608	8000.050603	12.243891	-0.052084	4.815569
249.704410	8000.036344	12.248896	-0.052104	4.815564
249.443517	8000.052394	12.253901	-0.052055	4.815570
249.682115	8000.092617	12.258906	-0.052100	4.815581
249.462336	8000.053803	12.263911	-0.052059	4.815570
249.370685	8000.069412	12.268915	-0.052042	4.815575
249.444348	8000.039661	12.273920	-0.052056	4.815566
249.280683	8000.016715	12.278925	-0.052026	4.815560
249.297019	8000.033019	12.283930	-0.052029	4.815565
249.243070	8000.033223	12.288935	-0.052019	4.815565
249.371675	8000.032136	12.293939	-0.052044	4.815564
249.429294	8000.050181	12.298944	-0.052055	4.815569
249.381153	8000.022713	12.303949	-0.052046	4.815562
249.352540	8000.029739	12.308954	-0.052041	4.815564
249.390260	8000.021828	12.313959	-0.052048	4.815561
249.349372	8000.047877	12.318963	-0.052040	4.815569
249.404241	8000.035974	12.323968	-0.052051	4.815565
249.514066	8000.040988	12.328973	-0.052072	4.815566
249.527709	8000.048704	12.333978	-0.052074	4.815568
249.267717	8000.024186	12.338983	-0.052026	4.815562
249.424297	8000.054526	12.343987	-0.052055	4.815571
249.465861	8000.048814	12.348992	-0.052063	4.815569
249.291242	8000.034233	12.353997	-0.052031	4.815565
249.428447	8000.038626	12.359002	-0.052057	4.815566
249.377375	8000.002567	12.364007	-0.052047	4.815556
249.351138	8000.049146	12.369011	-0.052043	4.815569
249.401950	8000.036109	12.374016	-0.052052	4.815565
249.504557	8000.052752	12.379021	-0.052072	4.815570
249.690510	8000.051533	12.384026	-0.052107	4.815568
249.344736	8000.029887	12.389031	-0.052042	4.815564
249.392617	8000.030686	12.394035	-0.052051	4.815564
249.409583	8000.009621	12.399040	-0.052055	4.815557
249.266994	8000.012650	12.404045	-0.052028	4.815559
249.344227	8000.033151	12.409050	-0.052043	4.815565
249.497779	8000.000432	12.414055	-0.052072	4.815554
249.607332	8000.060976	12.419059	-0.052092	4.815572
249.465114	8000.062943	12.424064	-0.052066	4.815573
249.451048	8000.030692	12.429069	-0.052064	4.815563
249.558374	8000.068772	12.434074	-0.052084	4.815574
249.352479	8000.022710	12.439079	-0.052046	4.815562
249.249721	8000.060564	12.444083	-0.052027	4.815573
249.288381	8000.038785	12.449088	-0.052034	4.815567
249.192752	7999.993456	12.454093	-0.052017	4.815554
249.186245	8000.039289	12.459098	-0.052016	4.815567
249.391989	8000.020237	12.464103	-0.052054	4.815561
249.389827	8000.014879	12.469107	-0.052054	4.815559
249.111041	8000.023162	12.474112	-0.052002	4.815563
249.259762	8000.008519	12.479117	-0.052030	4.815558
249.442026	8000.043549	12.484122	-0.052064	4.815567
249.331910	8000.027886	12.489127	-0.052044	4.815563
249.502187	8000.029614	12.494131	-0.052076	4.815563
249.648288	8000.037356	12.499136	-0.052103	4.815564
249.555597	8000.028385	12.504141	-0.052086	4.815562
249.628534	8000.071243	12.509146	-0.052100	4.815574
249.461040	8000.004448	12.514151	-0.052069	4.815556
249.479828	8000.031471	12.519155	-0.052073	4.815563
249.541725	8000.047450	12.524160	-0.052084	4.815568
249.540910	8000.031435	12.529165	-0.052084	4.815563
249.565742	8000.060692	12.534170	-0.052089	4.815572
249.464148	8000.035556	12.539175	-0.052070	4.815565
249.471731	8000.037833	12.544179	-0.052072	4.815565
249.535533	8000.048503	12.549184	-0.052084	4.815568
249.488814	8000.033874	12.554189	-0.052076	4.815564
249.668289	8000.057113	12.559194	-0.052109	4.815570
249.638815	8000.040629	12.564199	-0.052104	4.815565
249.740161	8000.065796	12.569203	-0.052123	4.815572
249.713512	8000.050427	12.574208	-0.052118	4.815568
249.712297	8000.051492	12.579213	-0.052118	4.815568
249.741070	8000.070135	12.584218	-0.052124	4.815573
249.608365	8000.026335	12.589223	-0.052099	4.815561
249.626169	8000.072565	12.594227	-0.052103	4.815575
249.618203	8000.071384	12.599232	-0.052102	4.815574
249.543842	8000.034945	12.604237	-0.052088	4.815564
249.526523	8000.063514	12.609242	-0.052085	4.815572
249.604209	8000.029557	12.614247	-0.052099	4.815562
249.775987	8000.044126	12.619251	-0.052132	4.815566
249.549183	8000.066072	12.624256	-0.052090	4.815573
249.656543	8000.049686	12.629261	-0.052110	4.815568
249.663838	8000.074386	12.634266	-0.052111	4.815575
249.440585	8000.024836	12.639271	-0.052070	4.815562
249.378249	8000.048399	12.644275	-0.052059	4.815569
249.566976	8000.048293	12.649280	-0.052094	4.815568
249.659553	8000.048753	12.654285	-0.052111	4.815567
249.649364	8000.053944	12.659290	-0.052110	4.815569
249.592334	8000.050894	12.664295	-0.052099	4.815568
249.693220	8000.065374	12.669299	-0.052118	4.815572
249.489948	8000.048189	12.674304	-0.052081	4.815568
249.553458	8000.030020	12.679309	-0.052093	4.815562
249.760174	8000.032344	12.684314	-0.052131	4.815562
249.770624	8000.023988	12.689319	-0.052133	4.815560
249.550164	8000.037494	12.694323	-0.052093	4.815565
249.613393	8000.039611	12.699328	-0.052105	4.815565
249.548164	8000.014000	12.704333	-0.052093	4.815558
249.571196	8000.056044	12.709338	-0.052097	4.815570
249.676254	8000.046029	12.714343	-0.052117	4.815567
249.730295	8000.068287	12.719347	-0.052127	4.815573
249.707067	8000.063654	12.724352	-0.052123	4.815572
249.509159	8000.041217	12.729357	-0.052086	4.815566
249.773610	8000.082930	12.734362	-0.052136	4.815577
249.597950	8000.058720	12.739367	-0.052103	4.815571
249.588026	8000.047895	12.744371	-0.052102	4.815567
249.826542	8000.074234	12.749376	-0.052146	4.815574
249.733233	8000.069524	12.754381	-0.052129	4.815573
249.698228	8000.098873	12.759386	-0.052123	4.815582
249.509848	8000.033873	12.764391	-0.052088	4.815564
249.801558	8000.079235	12.769395	-0.052142	4.815576
249.529730	8000.045979	12.774400	-0.052092	4.815567
249.427993	8000.031520	12.779405	-0.052073	4.815563
249.776300	8000.059650	12.784410	-0.052138	4.815570
249.891784	8000.057281	12.789415	-0.052160	4.815569
249.646291	8000.067174	12.794419	-0.052114	4.815573
249.490451	8000.068919	12.799424	-0.052086	4.815574
249.715786	8000.051256	12.804429	-0.052128	4.815568
249.772859	8000.068224	12.809434	-0.052139	4.815572
249.796231	8000.028040	12.814439	-0.052143	4.815561
249.775537	8000.048011	12.819443	-0.052139	4.815567
249.719537	8000.072745	12.824448	-0.052129	4.815574
249.589545	8000.032193	12.829453	-0.052105	4.815563
249.704603	8000.084283	12.834458	-0.052127	4.815577
249.729645	8000.068690	12.839463	-0.052132	4.815573
249.667728	8000.062356	12.844467	-0.052120	4.815571
249.927781	8000.095455	12.849472	-0.052169	4.815580
249.827882	8000.050054	12.854477	-0.052151	4.815567
249.781332	8000.077078	12.859482	-0.052142	4.815575
249.732412	8000.054937	12.864487	-0.052133	4.815569
249.612529	8000.052998	12.869491	-0.052111	4.815569
249.893865	8000.045860	12.874496	-0.052164	4.815565
249.612853	8000.039154	12.879501	-0.052112	4.815565
249.506420	8000.071608	12.884506	-0.052092	4.815575
249.472691	8000.058259	12.889511	-0.052086	4.815571
249.703598	8000.080202	12.894515	-0.052129	4.815576
249.685307	8000.087396	12.899520	-0.052126	4.815578
249.770825	8000.075994	12.904525	-0.052142	4.815575
249.692356	8000.105701	12.909530	-0.052128	4.815584
249.662444	8000.064647	12.914535	-0.052122	4.815572
249.630949	8000.079102	12.919539	-0.052116	4.815576
249.766447	8000.062107	12.924544	-0.052142	4.815571
249.733804	8000.060524	12.929549	-0.052136	4.815570
249.756716	8000.084410	12.934554	-0.052140	4.815577
249.775174	8000.055894	12.939559	-0.052144	4.815569
249.639277	8000.063304	12.944563	-0.052119	4.815572
249.732756	8000.090479	12.949568	-0.052137	4.815579
249.534720	7999.999690	12.954573	-0.052100	4.815553
249.665470	8000.066987	12.959578	-0.052124	4.815572
249.751382	8000.055591	12.964583	-0.052141	4.815569
249.606298	8000.090619	12.969587	-0.052114	4.815580
249.756305	8000.074930	12.974592	-0.052142	4.815574
249.830253	8000.053727	12.979597	-0.052156	4.815568
249.861200	8000.072405	12.984602	-0.052162	4.815573
249.865733	8000.032981	12.989607	-0.052163	4.815562
249.719728	8000.054110	12.994611	-0.052136	4.815568
249.855155	8000.079834	12.999616	-0.052161	4.815575
249.874770	8000.065219	13.004621	-0.052165	4.815571
250.030923	8000.082738	13.009626	-0.052194	4.815575
249.861094	8000.046875	13.014631	-0.052163	4.815566
249.869628	8000.054507	13.019635	-0.052165	4.815568
250.031544	8000.079596	13.024640	-0.052195	4.815574
249.597677	8000.031946	13.029645	-0.052115	4.815562
249.789409	8000.071405	13.034650	-0.052150	4.815573
249.739834	8000.064205	13.039655	-0.052141	4.815571
249.664333	8000.054446	13.044659	-0.052128	4.815569
249.608695	8000.080254	13.049664	-0.052117	4.815577
249.708521	8000.038114	13.054669	-0.052136	4.815564
249.918262	8000.089614	13.059674	-0.052175	4.815578
249.786201	8000.086407	13.064679	-0.052151	4.815577
249.691583	8000.074200	13.069683	-0.052134	4.815574
249.914897	8000.079999	13.074688	-0.052175	4.815575
249.796020	8000.037492	13.079693	-0.052153	4.815563
249.948484	8000.091262	13.084698	-0.052182	4.815578
249.788789	8000.049156	13.089703	-0.052153	4.815567
249.878128	8000.046360	13.094707	-0.052169	4.815565
249.948288	8000.059271	13.099712	-0.052183	4.815569
249.779485	8000.052260	13.104717	-0.052151	4.815567
250.071764	8000.084817	13.109722	-0.052206	4.815576
249.858751	8000.073880	13.114727	-0.052167	4.815573
249.849722	8000.076954	13.119731	-0.052165	4.815574
249.951191	8000.089308	13.124736	-0.052184	4.815577
249.708987	8000.050127	13.129741	-0.052139	4.815567
249.827454	8000.086254	13.134746	-0.052162	4.815577
250.058257	8000.078292	13.139751	-0.052205	4.815574
249.780336	8000.071635	13.144755	-0.052153	4.815573
249.910123	8000.091927	13.149760	-0.052177	4.815578
249.905435	8000.082256	13.154765	-0.052177	4.815576
250.132159	8000.101995	13.159770	-0.052219	4.815580
249.799015	8000.072009	13.164775	-0.052157	4.815573
249.755851	8000.059574	13.169779	-0.052150	4.815570
249.787498	8000.072924	13.174784	-0.052156	4.815573
249.545597	8000.036952	13.179789	-0.052111	4.815564
249.695878	8000.062918	13.184794	-0.052139	4.815571
249.784765	8000.032347	13.189799	-0.052156	4.815562
249.792034	8000.027143	13.194803	-0.052157	4.815560
249.856595	8000.037826	13.199808	-0.052169	4.815563
249.677537	8000.048804	13.204813	-0.052136	4.815567
249.985374	8000.082683	13.209818	-0.052194	4.815575
249.689500	8000.070393	13.214823	-0.052139	4.815573
249.724763	8000.083802	13.219827	-0.052146	4.815577
249.872199	8000.084090	13.224832	-0.052173	4.815576
249.803808	8000.056291	13.229837	-0.052161	4.815568
249.712199	8000.067629	13.234842	-0.052144	4.815572
249.937979	8000.049973	13.239847	-0.052186	4.815566
250.017331	8000.071577	13.244851	-0.052201	4.815572
250.127834	8000.085147	13.249856	-0.052222	4.815575
250.017879	8000.045989	13.254861	-0.052202	4.815564
250.003075	8000.067124	13.259866	-0.052199	4.815571
249.989555	8000.035949	13.264871	-0.052197	4.815562
249.799745	8000.057431	13.269875	-0.052162	4.815569
249.803747	8000.064989	13.274880	-0.052163	4.815571
249.840914	8000.058137	13.279885	-0.052170	4.815569
249.952128	8000.078126	13.284890	-0.052191	4.815574
249.820804	8000.058911	13.289895	-0.052166	4.815569
249.946951	8000.056716	13.294899	-0.052190	4.815568
249.810444	8000.066253	13.299904	-0.052165	4.815571
249.919933	8000.032814	13.304909	-0.052185	4.815561
250.109045	8000.087182	13.309914	-0.052221	4.815576
249.868020	8000.055497	13.314919	-0.052176	4.815568
249.529371	8000.063869	13.319923	-0.052113	4.815572
249.733038	8000.099250	13.324928	-0.052151	4.815581
249.972197	8000.039093	13.329933	-0.052196	4.815562
250.054206	8000.057537	13.334938	-0.052212	4.815567
249.902441	8000.055077	13.339943	-0.052184	4.815567
249.973544	8000.060527	13.344947	-0.052197	4.815569
249.958733	8000.061370	13.349952	-0.052194	4.815569
249.861480	8000.053391	13.354957	-0.052176	4.815567
249.920181	8000.069319	13.359962	-0.052188	4.815572
249.878671	8000.048367	13.364967	-0.052180	4.815566
249.752837	8000.039922	13.369971	-0.052157	4.815564
249.925367	8000.086543	13.374976	-0.052189	4.815577
249.926150	8000.055601	13.379981	-0.052189	4.815567
250.115487	8000.090750	13.384986	-0.052225	4.815577
250.075359	8000.064480	13.389991	-0.052218	4.815569
250.073406	8000.074077	13.394995	-0.052218	4.815572
250.182311	8000.072669	13.400000	-0.052238	4.815571
249.921575	8000.051341	13.405005	-0.052190	4.815566
249.852828	8000.065187	13.410010	-0.052177	4.815571
249.931749	8000.052609	13.415015	-0.052192	4.815567
249.974141	8000.050115	13.420019	-0.052200	4.815566
249.979845	8000.065177	13.425024	-0.052201	4.815570
250.126590	8000.076134	13.430029	-0.052229	4.815572
250.107654	8000.080114	13.435034	-0.052225	4.815574
250.039903	8000.064073	13.440039	-0.052213	4.815569
250.144706	8000.051918	13.445043	-0.052233	4.815565
250.093399	8000.075661	13.450048	-0.052223	4.815572
249.849698	8000.045000	13.455053	-0.052178	4.815565
249.745410	8000.063606	13.460058	-0.052159	4.815571
249.942393	8000.062567	13.465063	-0.052196	4.815569
249.957854	8000.059633	13.470067	-0.052199	4.815568
250.025753	8000.082118	13.475072	-0.052212	4.815575
250.012719	8000.054155	13.480077	-0.052210	4.815567
250.139914	8000.089357	13.485082	-0.052233	4.815576
249.990903	8000.055969	13.490087	-0.052206	4.815567
250.096639	8000.054509	13.495091	-0.052226	4.815566
250.264565	8000.076492	13.500096	-0.052257	4.815572
250.017272	8000.046840	13.505101	-0.052211	4.815564
249.990826	8000.078465	13.510106	-0.052207	4.815574
250.042027	8000.059026	13.515111	-0.052216	4.815568
250.047297	8000.063401	13.520115	-0.052218	4.815569
250.048395	8000.084796	13.525120	-0.052218	4.815575
249.898134	8000.056728	13.530125	-0.052190	4.815568
250.023319	8000.059858	13.535130	-0.052214	4.815568
249.830953	8000.048190	13.540135	-0.052178	4.815566
249.894099	8000.021471	13.545139	-0.052190	4.815557
250.058067	8000.074360	13.550144	-0.052221	4.815572
249.801226	8000.025329	13.555149	-0.052173	4.815559
249.905817	8000.044141	13.560154	-0.052193	4.815564
250.005770	8000.040451	13.565159	-0.052212	4.815562
249.807296	8000.052179	13.570163	-0.052175	4.815567
249.820370	8000.057750	13.575168	-0.052177	4.815568
249.931617	8000.045699	13.580173	-0.052198	4.815564
250.066214	8000.061798	13.585178	-0.052224	4.815568
250.050149	8000.024174	13.590183	-0.052221	4.815557
249.931318	8000.036134	13.595187	-0.052199	4.815562
250.382559	8000.056336	13.600192	-0.052283	4.815565
250.199014	8000.017044	13.605197	-0.052249	4.815555
250.125425	8000.052171	13.610202	-0.052236	4.815565
250.098858	8000.043211	13.615207	-0.052231	4.815563
249.705664	8000.059236	13.620211	-0.052158	4.815569
249.841488	8000.068946	13.625216	-0.052183	4.815572
249.992675	8000.030849	13.630221	-0.052212	4.815560
250.055776	8000.061800	13.635226	-0.052224	4.815568
249.988586	8000.012661	13.640231	-0.052211	4.815554
249.936972	8000.056690	13.645235	-0.052202	4.815567
250.127514	8000.069431	13.650240	-0.052238	4.815570
250.142257	8000.069689	13.655245	-0.052241	4.815570
250.154619	8000.068840	13.660250	-0.052243	4.815570
250.220688	8000.052848	13.665255	-0.052256	4.815565
250.189044	8000.042737	13.670259	-0.052250	4.815562
249.983093	8000.050071	13.675264	-0.052212	4.815565
249.944562	8000.038779	13.680269	-0.052205	4.815562
250.221550	8000.009144	13.685274	-0.052256	4.815552
249.989866	8000.048097	13.690279	-0.052214	4.815565
249.881641	8000.046347	13.695283	-0.052194	4.815565
249.728488	8000.066292	13.700288	-0.052165	4.815571
249.829530	8000.035919	13.705293	-0.052184	4.815562
249.539899	8000.066451	13.710298	-0.052131	4.815572
249.797112	8000.057852	13.715303	-0.052179	4.815568
249.777401	8000.036188	13.720307	-0.052175	4.815562
249.892478	8000.060511	13.725312	-0.052197	4.815569
249.926733	8000.017301	13.730317	-0.052203	4.815556
250.050518	8000.053514	13.735322	-0.052227	4.815566
250.149648	8000.053014	13.740327	-0.052245	4.815565
249.929094	8000.040886	13.745331	-0.052204	4.815563
250.065727	8000.051678	13.750336	-0.052230	4.815565
249.944575	8000.015542	13.755341	-0.052208	4.815555
249.780760	8000.035312	13.760346	-0.052177	4.815562
250.138561	8000.037967	13.765351	-0.052244	4.815561
250.176020	8000.022577	13.770355	-0.052251	4.815556
250.203778	8000.068971	13.775360	-0.052257	4.815570
250.146124	8000.027463	13.780365	-0.052246	4.815558
250.107683	8000.072776	13.785370	-0.052239	4.815571
250.158248	8000.055463	13.790375	-0.052249	4.815566
249.994612	8000.053876	13.795379	-0.052219	4.815566
250.231122	8000.062027	13.800384	-0.052263	4.815567
250.164988	8000.063100	13.805389	-0.052251	4.815568
249.924142	8000.069865	13.810394	-0.052206	4.815571
249.994617	8000.075305	13.815399	-0.052219	4.815572
250.173127	8000.052605	13.820403	-0.052253	4.815565
250.043338	8000.073999	13.825408	-0.052229	4.815572
249.940928	8000.020012	13.830413	-0.052210	4.815557
250.026357	8000.049192	13.835418	-0.052226	4.815565
250.294471	8000.062132	13.840423	-0.052276	4.815567
250.073337	8000.021158	13.845427	-0.052235	4.815556
250.238326	8000.081541	13.850432	-0.052266	4.815573
250.197052	8000.015737	13.855437	-0.052259	4.815554
249.918484	8000.051789	13.860442	-0.052207	4.815566
250.108595	8000.045298	13.865447	-0.052242	4.815563
250.149433	8000.029963	13.870451	-0.052250	4.815558
250.313311	8000.048676	13.875456	-0.052281	4.815563
249.903249	8000.025977	13.880461	-0.052205	4.815558
249.983925	8000.058283	13.885466	-0.052220	4.815567
250.264401	8000.050065	13.890471	-0.052272	4.815564
249.910397	8000.021874	13.895475	-0.052207	4.815557
250.025357	8000.049400	13.900480	-0.052228	4.815565
250.068979	8000.031973	13.905485	-0.052237	4.815559
250.142987	8000.031063	13.910490	-0.052251	4.815559
250.093450	8000.050563	13.915495	-0.052242	4.815565
250.162195	8000.063451	13.920499	-0.052255	4.815568
250.176908	8000.072252	13.925504	-0.052258	4.815571
249.954452	8000.049413	13.930509	-0.052216	4.815565
250.055169	8000.067095	13.935514	-0.052235	4.815570
250.053943	8000.063888	13.940519	-0.052235	4.815569
249.902777	8000.062505	13.945523	-0.052207	4.815569
249.936561	8000.079093	13.950528	-0.052214	4.815574
249.895642	8000.031451	13.955533	-0.052206	4.815560
249.825268	8000.068767	13.960538	-0.052193	4.815571
249.811852	8000.060021	13.965543	-0.052191	4.815569
249.813859	8000.053663	13.970547	-0.052192	4.815567
250.221337	8000.069946	13.975552	-0.052268	4.815570
250.020356	8000.064545	13.980557	-0.052231	4.815569
249.969734	8000.079756	13.985562	-0.052221	4.815574
250.208781	8000.096492	13.990567	-0.052266	4.815577
249.978879	8000.083143	13.995571	-0.052223	4.815575
250.036554	8000.107598	14.000576	-0.052234	4.815582
250.118169	8000.043801	14.005581	-0.052250	4.815562
250.193805	8000.079229	14.010586	-0.052264	4.815572
250.247240	8000.087595	14.015591	-0.052274	4.815575
250.223536	8000.061593	14.020595	-0.052270	4.815567
250.292843	8000.101190	14.025600	-0.052283	4.815578
250.084617	8000.070039	14.030605	-0.052245	4.815570
250.018883	8000.076458	14.035610	-0.052232	4.815572
250.200390	8000.073032	14.040615	-0.052266	4.815571
250.124301	8000.051515	14.045619	-0.052252	4.815565
250.190700	8000.076112	14.050624	-0.052265	4.815572
250.069346	8000.045312	14.055629	-0.052243	4.815563
250.045643	8000.079117	14.060634	-0.052238	4.815573
250.073154	8000.083856	14.065639	-0.052244	4.815574
250.087193	8000.083034	14.070643	-0.052247	4.815574
250.234394	8000.113223	14.075648	-0.052274	4.815582
250.020255	8000.057412	14.080653	-0.052234	4.815567
249.867581	8000.045324	14.085658	-0.052206	4.815564
250.104229	8000.058818	14.090663	-0.052251	4.815567
250.108212	8000.056764	14.095667	-0.052251	4.815566
250.202862	8000.056191	14.100672	-0.052269	4.815566
250.199173	8000.037992	14.105677	-0.052269	4.815560
250.155272	8000.063992	14.110682	-0.052261	4.815568
250.137681	8000.080810	14.115687	-0.052258	4.815573
249.955842	8000.047954	14.120691	-0.052224	4.815564
250.209185	8000.074536	14.125696	-0.052271	4.815571
250.325246	8000.057225	14.130701	-0.052293	4.815565
250.128995	8000.055105	14.135706	-0.052257	4.815566
250.232784	8000.063225	14.140711	-0.052276	4.815567
250.071779	8000.028573	14.145715	-0.052247	4.815558
250.272448	8000.059635	14.150720	-0.052284	4.815566
250.149848	8000.048039	14.155725	-0.052262	4.815563
250.277417	8000.073635	14.160730	-0.052286	4.815570
250.330137	8000.084125	14.165735	-0.052296	4.815573
250.216830	8000.067340	14.170739	-0.052275	4.815569
250.219798	8000.078085	14.175744	-0.052275	4.815572
250.210458	8000.072610	14.180749	-0.052274	4.815570
250.066437	8000.073479	14.185754	-0.052247	4.815571
250.291963	8000.068636	14.190759	-0.052289	4.815569
250.204728	8000.035189	14.195763	-0.052273	4.815559
250.105949	8000.066700	14.200768	-0.052255	4.815569
250.191131	8000.054225	14.205773	-0.052271	4.815565
250.258454	8000.084177	14.210778	-0.052284	4.815573
250.299330	8000.058162	14.215783	-0.052292	4.815566
249.920524	8000.057333	14.220787	-0.052221	4.815567
250.242990	8000.080772	14.225792	-0.052282	4.815572
250.145239	8000.050357	14.230797	-0.052264	4.815564
250.022785	8000.086823	14.235802	-0.052241	4.815575
250.236040	7999.284005	14.240807	-0.052280	4.815340

250.376193	7995.976006	14.245811	-0.052305	4.814372
250.423935	7990.567486	14.250816	-0.052310	4.812790
250.339142	7983.930516	14.255821	-0.052290	4.810849
250.398154	7976.566913	14.260826	-0.052297	4.808693
250.322815	7969.003033	14.265831	-0.052278	4.806479
249.995212	7961.109562	14.270835	-0.052212	4.804168
250.042106	7953.368413	14.275840	-0.052216	4.801899
250.100573	7945.352205	14.280845	-0.052222	4.799548
249.916001	7937.409720	14.285850	-0.052182	4.797219
249.920954	7929.428216	14.290855	-0.052178	4.794876
249.998799	7921.392150	14.295859	-0.052188	4.792516
249.960569	7913.338186	14.300864	-0.052176	4.790149
249.787866	7905.432866	14.305869	-0.052138	4.787826
249.846305	7897.379708	14.310874	-0.052144	4.785458
249.796068	7889.447846	14.315879	-0.052130	4.783124
249.644620	7881.367966	14.320883	-0.052097	4.780746
249.839901	7873.432414	14.325888	-0.052128	4.778408
249.690336	7865.413555	14.330893	-0.052095	4.776045
249.512267	7857.349664	14.335898	-0.052057	4.773669
249.502902	7849.387237	14.340903	-0.052050	4.771320
249.465417	7841.344840	14.345907	-0.052038	4.768947
249.573193	7833.409735	14.350912	-0.052053	4.766603
249.528475	7825.345641	14.355917	-0.052040	4.764221
249.349981	7817.410735	14.360922	-0.052002	4.761877
249.369842	7809.383976	14.365927	-0.052000	4.759503
249.112980	7801.384408	14.370931	-0.051947	4.757137
249.139377	7793.368936	14.375936	-0.051947	4.754764
249.318439	7785.299089	14.380941	-0.051976	4.752374
249.087122	7777.314079	14.385946	-0.051928	4.750009
249.085443	7769.318764	14.390951	-0.051922	4.747638
248.995107	7761.301259	14.395955	-0.051900	4.745261
249.198335	7753.325565	14.400960	-0.051933	4.742893
249.056207	7745.337659	14.405965	-0.051902	4.740522
249.077085	7737.372249	14.410970	-0.051901	4.738156
249.025118	7729.328189	14.415975	-0.051886	4.735765
248.627622	7721.283859	14.420979	-0.051807	4.733374
248.874684	7713.336884	14.425984	-0.051848	4.731010
249.003992	7705.313018	14.430989	-0.051867	4.728621
248.727295	7697.284270	14.435994	-0.051810	4.726231
248.730524	7689.278924	14.440999	-0.051806	4.723846
248.636632	7681.289357	14.446003	-0.051783	4.721464
248.596494	7673.279201	14.451008	-0.051771	4.719075
248.557073	7665.355763	14.456013	-0.051759	4.716711
248.587409	7657.285292	14.461018	-0.051759	4.714301
248.585188	7649.332583	14.466023	-0.051754	4.711926
248.400649	7641.231066	14.471027	-0.051714	4.709505
248.493004	7633.300782	14.476032	-0.051727	4.707133
248.422216	7625.289819	14.481037	-0.051708	4.704737
248.315765	7617.310876	14.486042	-0.051684	4.702349
248.306403	7609.295012	14.491047	-0.051677	4.699948
248.265323	7601.321587	14.496051	-0.051664	4.697560
248.367039	7593.291739	14.501056	-0.051678	4.695152
248.294276	7585.253433	14.506061	-0.051659	4.692741
248.211368	7577.247316	14.511066	-0.051639	4.690339
248.319932	7569.289093	14.516071	-0.051654	4.687949
247.884096	7561.225805	14.521075	-0.051568	4.685528
247.936667	7553.314943	14.526080	-0.051573	4.683150
248.067669	7545.323391	14.531085	-0.051592	4.680747
247.935178	7537.269192	14.536090	-0.051563	4.678324
247.920005	7529.289275	14.541095	-0.051555	4.675922
247.863618	7521.235552	14.546099	-0.051539	4.673496
247.839608	7513.145790	14.551104	-0.051530	4.671059
247.800124	7505.203068	14.556109	-0.051517	4.668664
247.799933	7497.194246	14.561114	-0.051512	4.666248
247.879183	7489.198168	14.566119	-0.051522	4.663835
247.661079	7481.232993	14.571123	-0.051476	4.661430
247.594197	7473.213675	14.576128	-0.051459	4.659007
247.650014	7465.296039	14.581133	-0.051464	4.656614
247.490672	7457.188782	14.586138	-0.051430	4.654162
247.329706	7449.238523	14.591143	-0.051395	4.651757
247.339331	7441.172302	14.596147	-0.051391	4.649315
247.345157	7433.255603	14.601152	-0.051387	4.646917
247.294398	7425.188377	14.606157	-0.051373	4.644472
247.331556	7417.234731	14.611162	-0.051375	4.642060
247.635104	7409.249745	14.616167	-0.051426	4.639638
247.290116	7401.263517	14.621171	-0.051357	4.637214
247.060586	7393.194441	14.626176	-0.051309	4.634763
247.155940	7385.185665	14.631181	-0.051322	4.632330
247.151554	7377.177865	14.636186	-0.051316	4.629895
247.187345	7369.180485	14.641191	-0.051318	4.627462
247.053157	7361.199465	14.646195	-0.051288	4.625034
247.084059	7353.244333	14.651200	-0.051289	4.622611
247.049114	7345.194987	14.656205	-0.051277	4.620159
246.835327	7337.193914	14.661210	-0.051232	4.617720
247.007937	7329.163422	14.666215	-0.051259	4.615271
247.068104	7321.155557	14.671219	-0.051266	4.612827
247.037454	7313.143769	14.676224	-0.051255	4.610381
247.037218	7305.185282	14.681229	-0.051250	4.607950
246.880713	7297.143286	14.686234	-0.051216	4.605492
246.723114	7289.211801	14.691239	-0.051181	4.603066
246.593102	7281.152942	14.696243	-0.051152	4.600601
246.799833	7273.186737	14.701248	-0.051185	4.598162
246.563673	7265.185591	14.706253	-0.051136	4.595711
246.580787	7257.135433	14.711258	-0.051135	4.593244
246.507057	7249.104020	14.716263	-0.051116	4.590782
246.443862	7241.109488	14.721267	-0.051099	4.588329
246.243894	7233.134822	14.726272	-0.051057	4.585881
246.185534	7225.135699	14.731277	-0.051041	4.583424
246.251724	7217.165963	14.736282	-0.051048	4.580975
246.403434	7209.141348	14.741287	-0.051072	4.578508
246.292020	7201.120785	14.746291	-0.051046	4.576041
246.363954	7193.141533	14.751296	-0.051054	4.573585
246.097773	7185.154520	14.756301	-0.051000	4.571126
246.083790	7177.044387	14.761306	-0.050992	4.568627
246.354552	7169.129991	14.766311	-0.051037	4.566187
246.227757	7161.087738	14.771315	-0.051009	4.563706
246.033075	7153.212014	14.776320	-0.050967	4.561276
245.977410	7145.131739	14.781325	-0.050952	4.558781
245.820365	7137.176599	14.786330	-0.050918	4.556323
245.813822	7129.141301	14.791335	-0.050912	4.553839
245.815288	7121.093203	14.796339	-0.050907	4.551350
245.774173	7113.085034	14.801344	-0.050894	4.548871
245.695181	7105.112705	14.806349	-0.050874	4.546403
245.618094	7097.082269	14.811354	-0.050855	4.543915
245.679876	7089.174294	14.816359	-0.050862	4.541464
245.727459	7081.101582	14.821363	-0.050865	4.538960
245.579049	7073.164263	14.826368	-0.050833	4.536497
245.692251	7065.131155	14.831373	-0.050849	4.534003
245.340023	7057.080335	14.836378	-0.050778	4.531501
245.613498	7049.139375	14.841383	-0.050824	4.529034
245.551093	7041.098573	14.846387	-0.050807	4.526533
245.522133	7033.098120	14.851392	-0.050797	4.524044
245.620222	7025.161317	14.856397	-0.050810	4.521573
245.516502	7017.098069	14.861402	-0.050786	4.519061
245.391592	7009.190727	14.866407	-0.050758	4.516596
245.392318	7001.084599	14.871411	-0.050753	4.514068
245.201179	6993.027577	14.876416	-0.050712	4.511554
245.223712	6985.068342	14.881421	-0.050711	4.509069
245.253125	6977.059480	14.886426	-0.050712	4.506567
245.062113	6969.085924	14.891431	-0.050671	4.504075
244.972713	6961.093012	14.896435	-0.050650	4.501575
245.081182	6953.079857	14.901440	-0.050665	4.499068
245.261255	6945.110352	14.906445	-0.050693	4.496573
245.026879	6937.033521	14.911450	-0.050645	4.494043
244.859614	6929.094138	14.916455	-0.050608	4.491554
244.916680	6921.021675	14.921459	-0.050614	4.489023
244.949840	6913.057439	14.926464	-0.050615	4.486524
244.982974	6905.055881	14.931469	-0.050616	4.484012
244.721520	6897.080735	14.936474	-0.050563	4.481506
244.901798	6889.067759	14.941479	-0.050591	4.478988
244.656674	6881.097545	14.946483	-0.050541	4.476480
244.701686	6873.078137	14.951488	-0.050544	4.473957
244.776296	6865.052999	14.956493	-0.050553	4.471431
244.479424	6856.994974	14.961498	-0.050492	4.468892
244.704055	6849.034663	14.966503	-0.050529	4.466383
244.736605	6841.012708	14.971507	-0.050530	4.463854
244.460704	6833.048427	14.976512	-0.050474	4.461339
244.448886	6825.023275	14.981517	-0.050467	4.458806
244.485535	6817.012968	14.986522	-0.050468	4.456275
244.516356	6809.035913	14.991527	-0.050469	4.453754
244.345958	6801.018555	14.996531	-0.050432	4.451218
244.350404	6792.979918	15.001536	-0.050428	4.448674
244.347124	6785.022873	15.006541	-0.050423	4.446154
244.253851	6776.983862	15.011546	-0.050400	4.443607
244.258624	6769.076182	15.016551	-0.050396	4.441100
244.193196	6761.060767	15.021555	-0.050379	4.438558
244.164923	6753.028811	15.026560	-0.050369	4.436009
244.140433	6745.016181	15.031565	-0.050359	4.433464
243.961789	6736.944548	15.036570	-0.050321	4.430899
244.060193	6728.955154	15.041575	-0.050334	4.428359
243.765997	6720.985869	15.046579	-0.050274	4.425823
243.765046	6712.984567	15.051584	-0.050269	4.423277
243.877217	6705.021465	15.056589	-0.050285	4.420741
243.591198	6696.983735	15.061594	-0.050227	4.418179
243.843425	6688.998296	15.066599	-0.050269	4.415634
243.702346	6680.950127	15.071603	-0.050237	4.413066
243.601103	6672.950078	15.076608	-0.050213	4.410512
243.576737	6665.021887	15.081613	-0.050204	4.407979
243.460497	6656.972791	15.086618	-0.050177	4.405407
243.563176	6649.041996	15.091623	-0.050191	4.402871
243.495214	6640.994672	15.096627	-0.050174	4.400296
243.405007	6633.022662	15.101632	-0.050152	4.397744
243.412446	6624.997155	15.106637	-0.050148	4.395173
243.395422	6616.939763	15.111642	-0.050140	4.392590
243.366336	6608.990496	15.116647	-0.050130	4.390041
243.305770	6600.970550	15.121651	-0.050113	4.387467
243.320397	6592.987059	15.126656	-0.050111	4.384904
243.334374	6585.047111	15.131661	-0.050109	4.382353
243.159672	6576.964708	15.136666	-0.050071	4.379754
243.252446	6569.026869	15.141671	-0.050083	4.377202
242.987878	6560.998412	15.146675	-0.050029	4.374616
242.868396	6552.992456	15.151680	-0.050002	4.372038
243.282911	6544.972473	15.156685	-0.050074	4.369456
243.152778	6537.008127	15.161690	-0.050045	4.366888
243.168742	6528.994430	15.166695	-0.050043	4.364303
242.934936	6521.054164	15.171699	-0.049994	4.361738
242.951664	6512.979418	15.176704	-0.049992	4.359130
242.748272	6505.054879	15.181709	-0.049949	4.356568
242.649363	6496.971807	15.186714	-0.049926	4.353954
242.819792	6488.861174	15.191719	-0.049952	4.351331
242.759847	6480.896010	15.196723	-0.049936	4.348752
242.616352	6472.909387	15.201728	-0.049905	4.346163
242.678991	6464.981066	15.206733	-0.049911	4.343594
242.564715	6456.962018	15.211738	-0.049885	4.340992
242.387232	6449.007838	15.216743	-0.049847	4.338410
242.492918	6441.018770	15.221747	-0.049862	4.335816
242.537434	6432.954118	15.226752	-0.049865	4.333196
242.405282	6424.937545	15.231757	-0.049835	4.330589
242.120072	6416.960886	15.236762	-0.049777	4.327992
242.623925	6408.955333	15.241767	-0.049866	4.325390
242.548204	6400.961622	15.246771	-0.049847	4.322786
242.277345	6392.971424	15.251776	-0.049791	4.320180
242.462633	6385.001622	15.256781	-0.049821	4.317583
242.344085	6376.938305	15.261786	-0.049794	4.314951
242.220510	6368.956555	15.266791	-0.049766	4.312344
242.029272	6360.882867	15.271795	-0.049725	4.309705
242.255434	6352.918956	15.276800	-0.049762	4.307103
242.136839	6344.944100	15.281805	-0.049735	4.304494
241.779222	6336.973178	15.286810	-0.049663	4.301882
242.072209	6328.959153	15.291815	-0.049713	4.299260
241.811706	6320.951934	15.296819	-0.049659	4.296634
241.805899	6312.915876	15.301824	-0.049653	4.293999
241.859665	6304.925146	15.306829	-0.049658	4.291378
241.852490	6296.920837	15.311834	-0.049652	4.288750
241.795841	6288.972090	15.316839	-0.049636	4.286139
241.721346	6280.942263	15.321843	-0.049618	4.283499
241.911453	6272.942947	15.326848	-0.049648	4.280870
241.733383	6264.961719	15.331853	-0.049610	4.278241
241.588439	6256.924909	15.336858	-0.049578	4.275594
241.890229	6248.910867	15.341863	-0.049629	4.272956
241.830728	6240.848667	15.346867	-0.049613	4.270297
241.740656	6232.898281	15.351872	-0.049591	4.267673
241.691067	6224.915823	15.356877	-0.049577	4.265038
241.571682	6216.942090	15.361882	-0.049550	4.262403
241.505773	6208.929406	15.366887	-0.049532	4.259754
241.407696	6200.960362	15.371891	-0.049509	4.257117
241.483670	6192.912314	15.376896	-0.049518	4.254454
241.333665	6184.936779	15.381901	-0.049485	4.251812
241.310968	6176.861008	15.386906	-0.049476	4.249136
241.304620	6168.934844	15.391911	-0.049470	4.246508
241.256573	6160.900945	15.396915	-0.049456	4.243842
241.098727	6152.927883	15.401920	-0.049421	4.241193
240.872740	6144.909207	15.406925	-0.049374	4.238527
241.159155	6136.931637	15.411930	-0.049423	4.235878
241.061370	6128.954123	15.416935	-0.049399	4.233224
240.766992	6120.887052	15.421939	-0.049339	4.230536
240.938718	6112.877156	15.426944	-0.049366	4.227870
241.063311	6104.920470	15.431949	-0.049385	4.225220
240.902543	6096.928548	15.436954	-0.049350	4.222554
240.855114	6088.965480	15.441959	-0.049336	4.219896
240.782906	6080.993245	15.446963	-0.049317	4.217234
240.651329	6072.977434	15.451968	-0.049288	4.214554
240.769457	6064.966632	15.456973	-0.049305	4.211878
240.740424	6056.912220	15.461978	-0.049294	4.209183
240.653554	6048.967335	15.466983	-0.049273	4.206523
240.599532	6040.926793	15.471987	-0.049258	4.203829
240.674458	6032.975866	15.476992	-0.049267	4.201165
240.561749	6024.943734	15.481997	-0.049241	4.198470
240.350829	6016.954332	15.487002	-0.049197	4.195787
240.487226	6008.888434	15.492007	-0.049217	4.193080
240.397874	6000.814498	15.497011	-0.049195	4.190366
240.195887	5992.855286	15.502016	-0.049153	4.187687
240.258204	5984.884331	15.507021	-0.049159	4.185006
240.360411	5976.931070	15.512026	-0.049174	4.182330
240.143855	5968.905321	15.517031	-0.049128	4.179624
240.002991	5960.945320	15.522035	-0.049097	4.176939
239.972149	5952.906355	15.527040	-0.049086	4.174227
239.963738	5944.918114	15.532045	-0.049080	4.171530
239.750838	5936.903113	15.537050	-0.049035	4.168821
239.753572	5928.919372	15.542055	-0.049030	4.166122
239.737764	5920.896222	15.547059	-0.049022	4.163409
239.537584	5912.922430	15.552064	-0.048980	4.160708
239.665526	5904.951839	15.557069	-0.048999	4.158010
239.620557	5896.884598	15.562074	-0.048986	4.155276
239.688500	5888.908044	15.567079	-0.048993	4.152572
239.691401	5880.869035	15.572083	-0.048989	4.149844
239.648381	5872.873699	15.577088	-0.048976	4.147129
239.879732	5864.879437	15.582093	-0.049014	4.144416
239.687069	5856.920999	15.587098	-0.048973	4.141707
239.708974	5848.901471	15.592103	-0.048972	4.138979
239.449540	5840.933091	15.597107	-0.048919	4.136264
239.312326	5832.903344	15.602112	-0.048888	4.133527
239.333171	5824.902537	15.607117	-0.048887	4.130800
239.227808	5816.859468	15.612122	-0.048862	4.128055
239.437339	5808.894361	15.617127	-0.048896	4.125339
239.097871	5800.918127	15.622131	-0.048828	4.122610
239.188022	5792.921341	15.627136	-0.048840	4.119878
239.410165	5784.960498	15.632141	-0.048876	4.117158
239.223830	5776.900678	15.637146	-0.048836	4.114397
238.924702	5768.873383	15.642151	-0.048776	4.111644
238.956300	5760.869125	15.647155	-0.048777	4.108901
238.825000	5752.863664	15.652160	-0.048747	4.106154
238.995270	5744.925752	15.657165	-0.048774	4.103433
239.037698	5736.903438	15.662170	-0.048777	4.100678
239.046166	5728.943218	15.667175	-0.048773	4.097943
238.773375	5720.951132	15.672179	-0.048717	4.095192
238.784955	5712.872716	15.677184	-0.048715	4.092412
238.933357	5704.902287	15.682189	-0.048737	4.089670
238.878338	5696.937015	15.687194	-0.048722	4.086924
238.691130	5688.954298	15.692199	-0.048682	4.084170
238.680656	5680.971827	15.697203	-0.048675	4.081415
238.574877	5672.957889	15.702208	-0.048650	4.078647
238.618305	5664.986808	15.707213	-0.048653	4.075894
238.478102	5656.935534	15.712218	-0.048622	4.073108
238.340892	5648.912266	15.717223	-0.048592	4.070331
238.334947	5640.930655	15.722227	-0.048586	4.067567
238.230796	5632.908051	15.727232	-0.048561	4.064787
238.379008	5625.014740	15.732237	-0.048584	4.062052
238.371897	5616.924392	15.737242	-0.048577	4.059246
238.421795	5608.991016	15.742247	-0.048582	4.056492
238.214547	5600.918317	15.747251	-0.048538	4.053685
238.168252	5592.915481	15.752256	-0.048524	4.050902
238.105580	5584.935905	15.757261	-0.048508	4.048126
237.998230	5576.936832	15.762266	-0.048483	4.045340
238.265085	5568.978483	15.767271	-0.048528	4.042571
237.924532	5560.952932	15.772275	-0.048459	4.039769
237.908248	5552.983609	15.777280	-0.048451	4.036989
238.079334	5544.954495	15.782285	-0.048478	4.034189
238.014428	5536.834784	15.787290	-0.048461	4.031351
237.786577	5528.892187	15.792295	-0.048413	4.028571
237.893794	5520.892363	15.797299	-0.048428	4.025775
237.959925	5512.894513	15.802304	-0.048436	4.022976
237.778228	5504.931835	15.807309	-0.048397	4.020184
237.639103	5496.939055	15.812314	-0.048366	4.017380
237.878104	5488.929777	15.817319	-0.048405	4.014575
237.853035	5480.903118	15.822323	-0.048396	4.011757
237.490662	5472.899014	15.827328	-0.048323	4.008939
237.651027	5464.946410	15.832333	-0.048348	4.006146
237.615662	5456.934504	15.837338	-0.048336	4.003328
237.463197	5448.943332	15.842343	-0.048303	4.000512
237.347429	5440.991621	15.847347	-0.048276	3.997709
237.357199	5432.951259	15.852352	-0.048273	3.994875
237.264361	5424.930173	15.857357	-0.048251	3.992044
237.119172	5416.880993	15.862362	-0.048219	3.989200
237.422681	5408.936958	15.867367	-0.048270	3.986399
237.339748	5400.922805	15.872371	-0.048250	3.983564
237.147800	5392.924789	15.877376	-0.048209	3.980732
237.132185	5384.966588	15.882381	-0.048201	3.977914
237.061305	5376.959384	15.887386	-0.048183	3.975076
236.942591	5368.943474	15.892391	-0.048156	3.972232
236.949226	5360.908049	15.897395	-0.048152	3.969382
236.916075	5352.952380	15.902400	-0.048141	3.966557
236.831537	5344.977632	15.907405	-0.048120	3.963722
236.924511	5336.967612	15.912410	-0.048132	3.960875
236.838794	5329.007912	15.917415	-0.048111	3.958042
236.846222	5320.985453	15.922419	-0.048108	3.955186
236.771675	5312.948260	15.927424	-0.048089	3.952321
236.616452	5304.966389	15.932429	-0.048055	3.949472
236.494713	5296.946725	15.937434	-0.048027	3.946608
236.363061	5288.997229	15.942439	-0.047998	3.943767
236.251654	5281.004488	15.947443	-0.047972	3.940909
236.251051	5273.008605	15.952448	-0.047967	3.938049
236.314597	5265.023186	15.957453	-0.047974	3.935193
236.157311	5256.979657	15.962458	-0.047939	3.932309
236.214539	5248.987923	15.967463	-0.047945	3.929446
236.103768	5241.015691	15.972467	-0.047919	3.926585
236.167509	5232.982230	15.977472	-0.047926	3.923702
236.358514	5225.048103	15.982477	-0.047957	3.920856
236.159460	5217.006724	15.987482	-0.047915	3.917962
236.329636	5209.013200	15.992487	-0.047941	3.915090
235.958376	5201.003026	15.997491	-0.047867	3.912199
235.959810	5192.986635	16.002496	-0.047862	3.909312
236.041034	5185.017921	16.007501	-0.047873	3.906440
235.934837	5176.988660	16.012506	-0.047848	3.903541
235.823480	5169.033970	16.017511	-0.047822	3.900667
235.915670	5161.023574	16.022515	-0.047834	3.897775
235.737682	5153.011718	16.027520	-0.047796	3.894874
235.664923	5145.032270	16.032525	-0.047777	3.891986
235.739771	5136.969096	16.037530	-0.047786	3.889067
235.714733	5129.053322	16.042535	-0.047777	3.886198
235.556776	5121.036911	16.047539	-0.047742	3.883288
235.702165	5113.029261	16.052544	-0.047764	3.880384
235.697891	5105.094017	16.057549	-0.047759	3.877502
235.345448	5097.007446	16.062554	-0.047688	3.874556
235.531520	5088.768495	16.067559	-0.047717	3.871562
235.461718	5080.857496	16.072563	-0.047699	3.868681
235.474941	5072.908497	16.077568	-0.047697	3.865786
235.495162	5064.965927	16.082573	-0.047696	3.862890
235.388636	5056.963563	16.087578	-0.047671	3.859968
235.177310	5049.030347	16.092583	-0.047626	3.857067
235.097064	5040.996882	16.097587	-0.047606	3.854130
235.163014	5033.005848	16.102592	-0.047614	3.851209
235.129738	5025.040874	16.107597	-0.047603	3.848294
234.685004	5016.989910	16.112602	-0.047515	3.845336
234.829902	5009.047663	16.117607	-0.047537	3.842428
234.972093	5001.033254	16.122611	-0.047558	3.839491
234.948222	4993.060649	16.127616	-0.047549	3.836564
234.828611	4985.084276	16.132621	-0.047521	3.833631
234.901747	4976.985973	16.137626	-0.047530	3.830655
234.782151	4969.057598	16.142631	-0.047503	3.827735
234.718298	4961.033829	16.147635	-0.047486	3.824779
234.742277	4953.073074	16.152640	-0.047485	3.821846
234.705431	4945.117699	16.157645	-0.047473	3.818911
234.496958	4937.080296	16.162650	-0.047430	3.815941
234.596180	4929.111671	16.167655	-0.047443	3.812999
234.474064	4921.057350	16.172659	-0.047415	3.810019
234.417067	4913.088258	16.177664	-0.047400	3.807070
234.332306	4905.094968	16.182669	-0.047379	3.804109
234.180847	4897.153134	16.187674	-0.047346	3.801163
234.368376	4889.119275	16.192679	-0.047376	3.798188
234.079591	4881.138308	16.197683	-0.047317	3.795220
234.159743	4873.056955	16.202688	-0.047327	3.792220
234.219156	4865.054569	16.207693	-0.047333	3.789247
233.979254	4857.082195	16.212698	-0.047283	3.786276
233.998173	4849.114929	16.217703	-0.047282	3.783311
233.925417	4841.104973	16.222707	-0.047263	3.780325
233.855768	4833.120447	16.227712	-0.047245	3.777346
233.893163	4825.091454	16.232717	-0.047247	3.774351
233.817961	4817.106577	16.237722	-0.047228	3.771367
233.942472	4809.105878	16.242727	-0.047246	3.768380
233.747611	4801.101783	16.247731	-0.047205	3.765381
233.846304	4793.119512	16.252736	-0.047218	3.762395
234.171200	4785.127971	16.257741	-0.047274	3.759409
233.794634	4777.196716	16.262746	-0.047199	3.756426
233.657035	4769.142382	16.267751	-0.047168	3.753401
233.580008	4761.109962	16.272755	-0.047148	3.750383
233.523581	4753.105185	16.277760	-0.047133	3.747373
233.581804	4745.113815	16.282765	-0.047139	3.744368
233.439747	4737.150502	16.287770	-0.047107	3.741367
233.657423	4729.156138	16.292775	-0.047143	3.738360
233.589225	4721.183648	16.297779	-0.047125	3.735352
233.385158	4713.160045	16.302784	-0.047082	3.732320
233.581327	4705.135036	16.307789	-0.047114	3.729293
233.422103	4697.151446	16.312794	-0.047079	3.726272
233.344587	4689.191469	16.317799	-0.047060	3.723259
233.354342	4681.192825	16.322803	-0.047056	3.720231
233.473195	4673.221697	16.327808	-0.047073	3.717213
233.183523	4665.232269	16.332813	-0.047015	3.714177
232.971413	4657.111295	16.337818	-0.046970	3.711089
233.134417	4649.123235	16.342823	-0.046995	3.708059
232.895890	4641.154584	16.347827	-0.046946	3.705024
232.888462	4633.177518	16.352832	-0.046939	3.701989
232.856644	4625.215154	16.357837	-0.046929	3.698956
232.913686	4617.209297	16.362842	-0.046934	3.695906
232.879788	4609.212733	16.367847	-0.046923	3.692856
232.902291	4601.201912	16.372851	-0.046922	3.689798
232.905351	4593.230052	16.377856	-0.046918	3.686753
232.760886	4585.243550	16.382861	-0.046886	3.683695
232.671843	4577.253539	16.387866	-0.046864	3.680635
232.786207	4569.292504	16.392871	-0.046880	3.677589
232.704364	4561.273800	16.397875	-0.046860	3.674513
232.464009	4553.258656	16.402880	-0.046810	3.671432
232.725210	4545.216614	16.407885	-0.046854	3.668351
232.558374	4537.236893	16.412890	-0.046818	3.665280
232.420161	4529.275796	16.417895	-0.046787	3.662215
232.404536	4521.267714	16.422899	-0.046779	3.659132
232.121142	4513.288664	16.427904	-0.046721	3.656051
232.025673	4505.285844	16.432909	-0.046699	3.652962
232.139240	4497.222973	16.437914	-0.046715	3.649854
232.348882	4489.271023	16.442919	-0.046749	3.646788
232.385923	4481.283463	16.447923	-0.046751	3.643701
232.101984	4473.310293	16.452928	-0.046693	3.640609
232.098843	4465.328626	16.457933	-0.046687	3.637518
231.925200	4457.310022	16.462938	-0.046650	3.634406
232.026594	4449.282449	16.467943	-0.046664	3.631295
232.097155	4441.268690	16.472947	-0.046672	3.628185
232.143766	4433.248993	16.477952	-0.046675	3.625071
232.052938	4425.312422	16.482957	-0.046654	3.621982
231.933816	4417.308490	16.487962	-0.046626	3.618863
231.878092	4409.342290	16.492967	-0.046611	3.615758
231.983819	4401.326719	16.497971	-0.046626	3.612636
231.645738	4393.305539	16.502976	-0.046558	3.609497
231.675777	4385.372371	16.507981	-0.046558	3.606399
231.687730	4377.337136	16.512986	-0.046555	3.603258
231.637541	4369.369184	16.517991	-0.046541	3.600139
231.473213	4361.398818	16.522995	-0.046506	3.597014
231.372995	4353.383076	16.528000	-0.046482	3.593869
231.532023	4345.385937	16.533005	-0.046506	3.590736
231.158845	4337.400010	16.538010	-0.046432	3.587590
231.370735	4329.366939	16.543015	-0.046466	3.584440
231.504773	4321.413940	16.548019	-0.046486	3.581315
231.251001	4313.429498	16.553024	-0.046434	3.578165
231.206412	4305.455931	16.558029	-0.046421	3.575022
231.183391	4297.427682	16.563034	-0.046411	3.571855
231.090522	4289.415651	16.568039	-0.046389	3.568690
230.939998	4281.438719	16.573043	-0.046356	3.565535
231.119792	4273.436639	16.578048	-0.046385	3.562376
231.162190	4265.445444	16.583053	-0.046387	3.559214
230.957207	4257.496242	16.588058	-0.046344	3.556060
231.101667	4249.402250	16.593063	-0.046366	3.552855
231.119087	4241.361939	16.598067	-0.046364	3.549665
230.909415	4233.397697	16.603072	-0.046320	3.546495
230.813596	4225.427426	16.608077	-0.046297	3.543324
230.691181	4217.428693	16.613082	-0.046270	3.540138
230.836865	4209.449137	16.618087	-0.046292	3.536964
230.650047	4201.467367	16.623091	-0.046252	3.533777
230.625501	4193.425841	16.628096	-0.046242	3.530568
230.654435	4185.493856	16.633101	-0.046243	3.527401
230.552838	4177.445421	16.638106	-0.046219	3.524181
230.641798	4169.504506	16.643111	-0.046230	3.521007
230.793947	4161.519121	16.648115	-0.046254	3.517814
230.523295	4153.529764	16.653120	-0.046198	3.514604
230.503874	4145.528509	16.658125	-0.046190	3.511394
230.465594	4137.473865	16.663130	-0.046177	3.508158
230.385999	4129.531584	16.668135	-0.046158	3.504964
230.125033	4121.596680	16.673139	-0.046104	3.501764
230.092076	4113.563082	16.678144	-0.046093	3.498528
230.276698	4105.581157	16.683149	-0.046122	3.495317
230.033055	4097.577270	16.688154	-0.046072	3.492081
230.087155	4089.543698	16.693159	-0.046077	3.488839
229.866323	4081.601696	16.698163	-0.046031	3.485622
229.832514	4073.594558	16.703168	-0.046020	3.482382
229.943204	4065.620491	16.708173	-0.046035	3.479157
229.921869	4057.649579	16.713178	-0.046026	3.475926
229.840141	4049.635491	16.718183	-0.046006	3.472673
229.942795	4041.562044	16.723187	-0.046020	3.469398
229.689515	4033.624343	16.728192	-0.045968	3.466164
229.784601	4025.617265	16.733197	-0.045981	3.462910
229.499622	4017.641958	16.738202	-0.045922	3.459654
229.594324	4009.662214	16.743207	-0.045935	3.456404
229.384227	4001.654779	16.748211	-0.045891	3.453131
229.443873	3993.631002	16.753216	-0.045897	3.449857
229.483805	3985.670621	16.758221	-0.045899	3.446604
229.352277	3977.678233	16.763226	-0.045870	3.443330
229.459036	3969.681786	16.768231	-0.045885	3.440060
229.250044	3961.733061	16.773235	-0.045841	3.436795
229.187924	3953.685697	16.778240	-0.045824	3.433491
229.318575	3945.697217	16.783245	-0.045844	3.430215
229.161907	3937.694313	16.788250	-0.045809	3.426920
228.985123	3929.727381	16.793255	-0.045772	3.423636
228.914329	3921.740509	16.798259	-0.045753	3.420344
228.891030	3913.754416	16.803264	-0.045744	3.417051
228.909452	3905.727213	16.808269	-0.045742	3.413739
228.998527	3897.701182	16.813274	-0.045754	3.410427
228.864339	3889.772412	16.818279	-0.045724	3.407144
228.923695	3881.734190	16.823283	-0.045730	3.403819
228.803786	3873.812925	16.828288	-0.045703	3.400534
228.882311	3865.829338	16.833293	-0.045712	3.397226
228.593456	3857.838454	16.838298	-0.045654	3.393899
228.594073	3849.718549	16.843303	-0.045649	3.390526
228.575970	3841.759867	16.848307	-0.045640	3.387215
228.655618	3833.762493	16.853312	-0.045650	3.383888
228.370221	3825.839052	16.858317	-0.045592	3.380577
228.447426	3817.835888	16.863322	-0.045601	3.377241
228.533836	3809.830100	16.868327	-0.045612	3.373901
228.341254	3801.833587	16.873331	-0.045571	3.370552
228.165990	3793.859300	16.878336	-0.045534	3.367210
228.383597	3785.884709	16.883341	-0.045569	3.363878
228.020907	3777.918595	16.888346	-0.045497	3.360526
228.217534	3769.912495	16.893351	-0.045528	3.357173
228.210042	3761.908870	16.898355	-0.045522	3.353811
228.182089	3753.860128	16.903360	-0.045512	3.350426
228.181172	3745.909129	16.908365	-0.045507	3.347080
228.183955	3737.881331	16.913370	-0.045502	3.343698
228.242847	3729.915969	16.918375	-0.045508	3.340341
228.084646	3721.991560	16.923379	-0.045474	3.336989
228.028224	3713.955537	16.928384	-0.045458	3.333591
228.171488	3705.941235	16.933389	-0.045480	3.330207
228.018562	3697.947007	16.938394	-0.045446	3.326816
227.711187	3689.992994	16.943399	-0.045384	3.323433
227.705130	3682.013317	16.948403	-0.045378	3.320047
227.820739	3674.011205	16.953408	-0.045394	3.316652
227.846156	3666.006137	16.958413	-0.045394	3.313249
227.634778	3657.998036	16.963418	-0.045350	3.309833
227.609331	3650.004479	16.968423	-0.045340	3.306426
227.533555	3642.033903	16.973427	-0.045321	3.303024
227.379493	3634.027412	16.978432	-0.045287	3.299600
227.560487	3626.071603	16.983437	-0.045316	3.296206
227.448765	3618.056800	16.988442	-0.045290	3.292773
227.263590	3610.062116	16.993447	-0.045250	3.289342
227.352722	3602.102105	16.998451	-0.045262	3.285933
227.244761	3594.112851	17.003456	-0.045237	3.282500
227.303700	3586.126354	17.008461	-0.045243	3.279071
227.280957	3578.146158	17.013466	-0.045234	3.275638
227.010351	3570.135980	17.018471	-0.045178	3.272179
227.236343	3562.115984	17.023475	-0.045215	3.268731
226.926562	3554.145992	17.028480	-0.045153	3.265280
227.049329	3546.194159	17.033485	-0.045171	3.261851
227.052583	3538.196629	17.038490	-0.045166	3.258393
226.901503	3530.191481	17.043495	-0.045133	3.254923
226.809830	3522.189481	17.048499	-0.045111	3.251452
226.717594	3514.191090	17.053504	-0.045089	3.247979
226.696841	3506.218412	17.058509	-0.045080	3.244516
226.600050	3498.249094	17.063514	-0.045057	3.241048
226.625471	3490.265544	17.068519	-0.045057	3.237575
226.834781	3482.266292	17.073523	-0.045091	3.234099
226.612963	3474.171885	17.078528	-0.045044	3.230561
226.702965	3466.210304	17.083533	-0.045056	3.227089
226.722833	3458.203837	17.088538	-0.045055	3.223590
226.504814	3450.266868	17.093543	-0.045009	3.220109
226.307836	3442.305981	17.098547	-0.044967	3.216614
226.430798	3434.283875	17.103552	-0.044985	3.213102
226.370678	3426.316189	17.108557	-0.044969	3.209602
226.063759	3418.359248	17.113562	-0.044907	3.206093
226.271058	3410.335517	17.118567	-0.044940	3.202572
226.312914	3402.364554	17.123571	-0.044943	3.199064
226.276500	3394.390651	17.128576	-0.044931	3.195547
226.345352	3386.378755	17.133581	-0.044939	3.192014
226.197483	3378.384385	17.138586	-0.044907	3.188475
225.926213	3370.391727	17.143591	-0.044851	3.184928
225.914767	3362.447319	17.148595	-0.044844	3.181410
225.895668	3354.436430	17.153600	-0.044835	3.177857
225.965437	3346.454781	17.158605	-0.044843	3.174318
225.714842	3338.438462	17.163610	-0.044792	3.170746
225.740781	3330.456487	17.168615	-0.044792	3.167196
225.755246	3322.489466	17.173619	-0.044789	3.163649
225.529290	3314.507112	17.178624	-0.044742	3.160080
225.655834	3306.561837	17.183629	-0.044761	3.156540
225.731120	3298.500526	17.188634	-0.044770	3.152941
225.482572	3290.513472	17.193639	-0.044718	3.149357
225.658735	3282.515697	17.198643	-0.044746	3.145783
225.601425	3274.538669	17.203648	-0.044731	3.142204
225.684431	3266.554900	17.208653	-0.044741	3.138624
225.399066	3258.607413	17.213658	-0.044683	3.135040
225.344980	3250.599896	17.218663	-0.044668	3.131435
225.381792	3242.603043	17.223667	-0.044670	3.127835
225.225870	3234.596398	17.228672	-0.044636	3.124217
225.134013	3226.669469	17.233677	-0.044614	3.120635
225.285193	3218.668869	17.238682	-0.044637	3.117025
225.012980	3210.691336	17.243687	-0.044581	3.113403
225.019118	3202.670671	17.248691	-0.044577	3.109770
224.954493	3194.687776	17.253696	-0.044560	3.106146
225.014086	3186.701794	17.258701	-0.044566	3.102522
224.898234	3178.728988	17.263706	-0.044540	3.098892
224.918478	3170.764930	17.268711	-0.044538	3.095268
225.015553	3162.728508	17.273715	-0.044551	3.091611
224.758271	3154.759185	17.278720	-0.044498	3.087963
224.618620	3146.789569	17.283725	-0.044467	3.084316
224.574541	3138.827277	17.288730	-0.044454	3.080673
224.456781	3130.845788	17.293735	-0.044427	3.077013
224.664932	3122.803290	17.298739	-0.044461	3.073336
224.371611	3114.741173	17.303744	-0.044401	3.069622
224.489848	3106.781405	17.308749	-0.044418	3.065970
224.118603	3098.834314	17.313754	-0.044344	3.062296
224.283688	3090.843366	17.318759	-0.044370	3.058623
224.318987	3082.896904	17.323763	-0.044372	3.054960
224.348260	3074.860567	17.328768	-0.044372	3.051251
224.069255	3066.922438	17.333773	-0.044315	3.047568
224.151382	3058.927793	17.338778	-0.044325	3.043871
224.053287	3050.964146	17.343783	-0.044302	3.040176
224.178229	3042.997215	17.348787	-0.044320	3.036485
224.126141	3034.972983	17.353792	-0.044306	3.032755
224.116431	3026.989127	17.358797	-0.044299	3.029041
224.019507	3019.005395	17.363802	-0.044276	3.025319
223.696066	3011.053174	17.368807	-0.044211	3.021595
223.899161	3003.070574	17.373811	-0.044243	3.017878
223.825623	2995.059264	17.378816	-0.044225	3.014130
223.788838	2987.078768	17.383821	-0.044213	3.010393
223.566179	2979.105106	17.388826	-0.044166	3.006646
223.589084	2971.114305	17.393831	-0.044166	3.002898
223.573802	2963.158089	17.398835	-0.044158	2.999160
223.388439	2955.187328	17.403840	-0.044118	2.995401
223.441284	2947.153078	17.408845	-0.044123	2.991620
223.470979	2939.138693	17.413850	-0.044124	2.987843
223.537716	2931.139743	17.418855	-0.044131	2.984069
223.569141	2923.214696	17.423859	-0.044132	2.980325
223.506607	2915.233155	17.428864	-0.044115	2.976544
223.253766	2907.274887	17.433869	-0.044063	2.972759
222.886483	2899.281282	17.438874	-0.043990	2.968947
222.976333	2891.273399	17.443879	-0.044001	2.965147
222.925553	2883.339375	17.448883	-0.043987	2.961369
222.863356	2875.351237	17.453888	-0.043970	2.957561
222.887675	2867.345777	17.458893	-0.043970	2.953744
223.046798	2859.313880	17.463898	-0.043995	2.949916
222.926904	2851.343399	17.468903	-0.043967	2.946098
222.815336	2843.396744	17.473907	-0.043941	2.942287
222.840020	2835.406604	17.478912	-0.043941	2.938457
222.784933	2827.438147	17.483917	-0.043926	2.934628
222.627695	2819.448418	17.488922	-0.043891	2.930779
222.725288	2811.451167	17.493927	-0.043905	2.926935
222.857308	2803.498149	17.498931	-0.043924	2.923109
222.496270	2795.509302	17.503936	-0.043852	2.919234
222.510495	2787.573342	17.508941	-0.043850	2.915399
222.425412	2779.492397	17.513946	-0.043829	2.911484
222.441314	2771.481422	17.518951	-0.043827	2.907603
222.514727	2763.528801	17.523955	-0.043835	2.903749
222.373259	2755.569356	17.528960	-0.043804	2.899874
222.287480	2747.627284	17.533965	-0.043783	2.896006
222.172042	2739.626152	17.538970	-0.043757	2.892101
222.246007	2731.612920	17.543975	-0.043765	2.888196
222.141210	2723.662958	17.548979	-0.043741	2.884307
221.860285	2715.726828	17.553984	-0.043684	2.880410
221.975230	2707.742086	17.558989	-0.043700	2.876506
221.968283	2699.717518	17.563994	-0.043694	2.872569
221.980011	2691.716469	17.568999	-0.043691	2.868640
221.900812	2683.758151	17.574003	-0.043671	2.864722
221.926199	2675.776830	17.579008	-0.043671	2.860792
221.902500	2667.830336	17.584013	-0.043661	2.856872
221.775108	2659.823707	17.589018	-0.043633	2.852911
221.783001	2651.833161	17.594023	-0.043629	2.848960
221.897534	2643.868708	17.599027	-0.043645	2.845022
221.555158	2635.922381	17.604032	-0.043577	2.841062
221.628408	2627.941349	17.609037	-0.043585	2.837103
221.557640	2619.954561	17.614042	-0.043567	2.833127
221.307144	2611.947518	17.619047	-0.043515	2.829125
221.399683	2603.957179	17.624051	-0.043528	2.825145
221.217702	2596.008201	17.629056	-0.043489	2.821165
221.360675	2588.039543	17.634061	-0.043510	2.817188
221.159279	2580.053687	17.639066	-0.043468	2.813177
221.153605	2572.061804	17.644071	-0.043462	2.809168
221.091759	2564.093390	17.649075	-0.043445	2.805162
220.977335	2556.139355	17.654080	-0.043419	2.801155
221.278966	2548.125772	17.659085	-0.043470	2.797136
221.249054	2540.135320	17.664090	-0.043460	2.793104
221.091596	2532.155769	17.669095	-0.043425	2.789064
220.926509	2524.207870	17.674099	-0.043390	2.785033
221.110136	2516.218687	17.679104	-0.043419	2.780996
220.860574	2508.289014	17.684109	-0.043367	2.776958
220.610095	2500.314633	17.689114	-0.043316	2.772892
220.684102	2492.296990	17.694119	-0.043324	2.768816
220.689430	2484.327922	17.699123	-0.043320	2.764755
220.486551	2476.376639	17.704128	-0.043278	2.760685
220.547098	2468.409909	17.709133	-0.043284	2.756617
220.703629	2460.340002	17.714138	-0.043308	2.752496
220.550920	2452.336187	17.719143	-0.043275	2.748383
220.510172	2444.380436	17.724147	-0.043262	2.744296
220.276256	2436.441804	17.729152	-0.043213	2.740200
220.369601	2428.483074	17.734157	-0.043226	2.736107
220.269365	2420.487179	17.739162	-0.043202	2.731978
220.300086	2412.509007	17.744167	-0.043203	2.727859
220.419542	2404.537731	17.749171	-0.043220	2.723743
220.197998	2396.582355	17.754176	-0.043174	2.719608
220.318379	2388.623625	17.759181	-0.043191	2.715486
219.983486	2380.672527	17.764186	-0.043124	2.711333
219.922884	2372.648194	17.769191	-0.043108	2.707153
220.126018	2364.669276	17.774195	-0.043140	2.703007
219.836524	2356.726430	17.779200	-0.043082	2.698842
219.769961	2348.765593	17.784205	-0.043064	2.694675
219.664755	2340.775299	17.789210	-0.043040	2.690484
219.672713	2332.803473	17.794215	-0.043036	2.686304
219.822655	2324.827472	17.799219	-0.043059	2.682123
219.639128	2316.885832	17.804224	-0.043020	2.677933
219.737805	2308.885781	17.809229	-0.043033	2.673724
219.717257	2300.877294	17.814234	-0.043024	2.669496
219.568693	2292.901806	17.819239	-0.042992	2.665270
219.402085	2284.976599	17.824243	-0.042956	2.661063
219.225216	2277.011741	17.829248	-0.042918	2.656828
219.256028	2269.022538	17.834253	-0.042919	2.652586
219.256974	2261.025710	17.839258	-0.042914	2.648332
219.265796	2253.053932	17.844263	-0.042910	2.644085
219.280329	2245.104774	17.849267	-0.042908	2.639843
219.070358	2237.158663	17.854272	-0.042864	2.635581
219.051643	2229.157965	17.859277	-0.042855	2.631296
219.114354	2221.164035	17.864282	-0.042862	2.627013
219.006223	2213.208581	17.869287	-0.042837	2.622732
218.906044	2205.271276	17.874291	-0.042813	2.618454
218.788432	2197.299964	17.879296	-0.042786	2.614150
218.991459	2189.284390	17.884301	-0.042819	2.609837
218.752617	2181.345862	17.889306	-0.042770	2.605528
218.736944	2173.374076	17.894311	-0.042762	2.601209
218.781785	2165.433567	17.899315	-0.042765	2.596904
218.626601	2157.343219	17.904320	-0.042731	2.592496
218.668423	2149.284741	17.909325	-0.042734	2.588112
218.777171	2141.341326	17.914330	-0.042749	2.583788
218.644418	2133.422048	17.919335	-0.042720	2.579453
218.625092	2125.483363	17.924339	-0.042711	2.575108
218.596803	2117.508273	17.929344	-0.042701	2.570736
218.339179	2109.576831	17.934349	-0.042648	2.566363
218.307387	2101.637044	17.939354	-0.042637	2.561995
218.269710	2093.679284	17.944359	-0.042625	2.557608
218.295878	2085.707034	17.949363	-0.042625	2.553211
218.234375	2077.715330	17.954368	-0.042608	2.548789
218.039598	2069.769675	17.959373	-0.042567	2.544375
217.966184	2061.827811	17.964378	-0.042548	2.539965
218.148631	2053.831234	17.969383	-0.042577	2.535534
217.960314	2045.888574	17.974387	-0.042537	2.531099
217.985464	2037.892650	17.979392	-0.042537	2.526642
218.140475	2029.927684	17.984397	-0.042561	2.522204
218.011354	2021.988555	17.989402	-0.042532	2.517752
217.795496	2014.010419	17.994407	-0.042487	2.513264
217.964692	2006.004897	17.999411	-0.042513	2.508781
217.798370	1998.027977	18.004416	-0.042477	2.504281
217.712032	1990.111063	18.009421	-0.042456	2.499812
217.676248	1982.159005	18.014426	-0.042444	2.495320
217.562576	1974.162160	18.019431	-0.042418	2.490788
217.665258	1966.208032	18.024435	-0.042432	2.486288
217.422766	1958.264416	18.029440	-0.042382	2.481761
217.392958	1950.326710	18.034445	-0.042372	2.477244
217.342732	1942.331703	18.039450	-0.042357	2.472685
217.164710	1934.366762	18.044455	-0.042319	2.468125
217.161664	1926.410158	18.049459	-0.042314	2.463574
217.071395	1918.455976	18.054464	-0.042292	2.459010
217.083123	1910.507599	18.059469	-0.042289	2.454448
217.138543	1902.501003	18.064474	-0.042294	2.449848
216.851071	1894.579070	18.069479	-0.042236	2.445261
216.878354	1886.639956	18.074483	-0.042236	2.440680
216.941566	1878.652745	18.079488	-0.042243	2.436066
217.046306	1870.604629	18.084493	-0.042257	2.431410
216.959856	1862.644656	18.089498	-0.042236	2.426782
216.705650	1854.717015	18.094503	-0.042184	2.422152
216.799110	1846.770396	18.099507	-0.042196	2.417528
216.666636	1838.808533	18.104512	-0.042167	2.412868
216.756949	1830.825323	18.109517	-0.042178	2.408205
216.588179	1822.896776	18.114522	-0.042142	2.403544
216.515830	1814.950146	18.119527	-0.042124	2.398871
216.588509	1807.004981	18.124531	-0.042132	2.394202
216.417044	1799.015587	18.129536	-0.042095	2.389477
216.376613	1791.066525	18.134541	-0.042083	2.384778
216.356636	1783.126718	18.139546	-0.042074	2.380076
216.301401	1775.163429	18.144551	-0.042059	2.375349
215.924331	1767.241440	18.149555	-0.041983	2.370610
216.036885	1759.236094	18.154560	-0.041999	2.365852
216.180533	1751.291709	18.159565	-0.042021	2.361123
216.033297	1743.371108	18.164570	-0.041989	2.356376
215.992966	1735.363346	18.169575	-0.041976	2.351575
215.994138	1727.384256	18.174579	-0.041972	2.346785
215.555677	1719.464719	18.179584	-0.041885	2.341985
215.574364	1711.518772	18.184589	-0.041883	2.337196
215.563684	1703.550225	18.189594	-0.041876	2.332382
215.420511	1695.591435	18.194599	-0.041845	2.327553
215.489154	1687.639389	18.199603	-0.041853	2.322735
215.448118	1679.705933	18.204608	-0.041840	2.317910
215.293100	1671.747763	18.209613	-0.041806	2.313049
215.223910	1663.789295	18.214618	-0.041788	2.308186
215.287637	1655.812074	18.219623	-0.041795	2.303312
215.298750	1647.889689	18.224627	-0.041792	2.298457
215.338180	1639.915651	18.229632	-0.041795	2.293562
215.307596	1631.959878	18.234637	-0.041784	2.288662
215.225091	1624.025529	18.239642	-0.041764	2.283760
215.207309	1616.072585	18.244647	-0.041755	2.278842
215.028305	1608.148783	18.249651	-0.041717	2.273917
214.955009	1600.113357	18.254656	-0.041698	2.268922
214.888391	1592.183440	18.259661	-0.041681	2.263981
214.644580	1584.279965	18.264666	-0.041630	2.259031
214.739999	1576.297406	18.269671	-0.041643	2.254050
214.706108	1568.343446	18.274675	-0.041632	2.249065
214.584577	1560.406435	18.279680	-0.041604	2.244071
214.438862	1552.485331	18.284685	-0.041572	2.239074
214.599743	1544.512676	18.289690	-0.041597	2.234061
214.512937	1536.557188	18.294695	-0.041576	2.229025
214.457782	1528.623162	18.299699	-0.041561	2.223994
214.327186	1520.693635	18.304704	-0.041532	2.218948
214.273620	1512.762327	18.309709	-0.041517	2.213896
214.151956	1504.810817	18.314714	-0.041489	2.208814
213.992978	1496.861474	18.319719	-0.041454	2.203718
214.128352	1488.923379	18.324723	-0.041475	2.198644
214.008394	1480.978407	18.329728	-0.041447	2.193530
214.036805	1473.001484	18.334733	-0.041448	2.188398
214.046542	1465.045401	18.339738	-0.041444	2.183265
213.874637	1457.121728	18.344743	-0.041407	2.178124
213.721734	1449.218256	18.349747	-0.041374	2.172986
213.720100	1441.240068	18.354752	-0.041369	2.167801
213.744661	1433.307615	18.359757	-0.041368	2.162636
213.697854	1425.383725	18.364762	-0.041355	2.157458
213.529976	1417.447105	18.369767	-0.041318	2.152247
213.546374	1409.511762	18.374771	-0.041316	2.147042
213.409298	1401.569737	18.379776	-0.041286	2.141805
213.356082	1393.643226	18.384781	-0.041271	2.136574
213.569766	1385.659127	18.389786	-0.041306	2.131317
213.386891	1377.725942	18.394791	-0.041267	2.126043
213.398333	1369.814377	18.399795	-0.041264	2.120789
213.240652	1361.894806	18.404800	-0.041230	2.115500
213.295846	1353.877988	18.409805	-0.041235	2.110153
213.186869	1345.962003	18.414810	-0.041210	2.104845
212.863764	1338.052441	18.419815	-0.041145	2.099506
213.316305	1330.077644	18.424819	-0.041224	2.094186
213.092320	1322.153467	18.429824	-0.041177	2.088820
213.053158	1314.234691	18.434829	-0.041165	2.083462
213.014503	1306.324490	18.439834	-0.041153	2.078096
212.700705	1298.416567	18.444839	-0.041089	2.072690
212.607397	1290.477408	18.449843	-0.041067	2.067271
212.687263	1282.515097	18.454848	-0.041077	2.061839
212.808282	1274.583819	18.459853	-0.041094	2.056418
212.490994	1266.681497	18.464858	-0.041030	2.050959
212.452131	1258.737179	18.469863	-0.041018	2.045484
212.547594	1250.813367	18.474867	-0.041031	2.040022
212.382542	1242.911396	18.479872	-0.040995	2.034534
212.522681	1234.925497	18.484877	-0.041016	2.029004
212.440091	1227.004382	18.489882	-0.040996	2.023482
212.273403	1219.102165	18.494887	-0.040960	2.017948
212.449923	1211.144701	18.499891	-0.040988	2.012397
212.259499	1203.235152	18.504896	-0.040947	2.006825
211.971434	1195.355523	18.509901	-0.040889	2.001249
212.060827	1187.429221	18.514906	-0.040901	1.995664
211.923207	1179.496866	18.519911	-0.040870	1.990035
212.102410	1171.551529	18.524915	-0.040898	1.984414
211.792482	1163.668130	18.529920	-0.040836	1.978769
211.666649	1155.755089	18.534925	-0.040807	1.973107
211.701008	1147.800409	18.539930	-0.040809	1.967415
211.774079	1139.874405	18.544935	-0.040817	1.961732
211.690852	1131.989060	18.549939	-0.040797	1.956045
211.637110	1124.021906	18.554944	-0.040782	1.950285
211.597430	1116.090392	18.559949	-0.040770	1.944536
211.552826	1108.199383	18.564954	-0.040756	1.938798
211.257231	1100.304280	18.569959	-0.040696	1.933013
211.349052	1092.369087	18.574963	-0.040708	1.927224
211.092606	1084.478933	18.579968	-0.040656	1.921411
211.099315	1076.568406	18.584973	-0.040652	1.915596
211.104812	1068.637243	18.589978	-0.040648	1.909747
210.990761	1060.715162	18.594983	-0.040622	1.903874
210.874156	1052.837720	18.599987	-0.040595	1.898015
210.827134	1044.907933	18.604992	-0.040582	1.892107
210.792610	1036.985155	18.609997	-0.040570	1.886187
210.753144	1029.093614	18.615002	-0.040558	1.880271
210.745769	1021.198577	18.620007	-0.040552	1.874338
210.734334	1013.269791	18.625011	-0.040544	1.868360
210.675368	1005.346828	18.630016	-0.040528	1.862361
210.539368	997.467971	18.635021	-0.040498	1.856368
210.616594	989.537538	18.640026	-0.040508	1.850341
210.667980	981.620474	18.645031	-0.040512	1.844301
210.705293	973.749931	18.650035	-0.040514	1.838276
210.528484	965.857560	18.655040	-0.040476	1.832188
210.534062	957.944660	18.660045	-0.040472	1.826086
210.437593	950.062817	18.665050	-0.040450	1.819976
210.186470	942.201055	18.670055	-0.040398	1.813841
210.092609	934.307761	18.675059	-0.040375	1.807681
210.053839	926.404188	18.680064	-0.040363	1.801498
210.071197	918.504939	18.685069	-0.040362	1.795303
210.013330	910.559831	18.690074	-0.040346	1.789042
209.780545	902.691014	18.695079	-0.040297	1.782798
209.742685	894.815888	18.700083	-0.040286	1.776551
209.542445	886.926153	18.705088	-0.040243	1.770250
209.769014	878.999674	18.710093	-0.040280	1.763950
209.658302	871.137751	18.715098	-0.040255	1.757638
209.476015	863.264928	18.720103	-0.040216	1.751284
209.491457	855.378083	18.725107	-0.040214	1.744922
209.460827	847.495416	18.730112	-0.040203	1.738533
209.401403	839.624750	18.735117	-0.040187	1.732127
209.134755	831.767436	18.740122	-0.040133	1.725682
209.140683	823.889029	18.745127	-0.040129	1.719230
209.302814	815.985985	18.750131	-0.040154	1.712753
208.991199	808.120636	18.755136	-0.040091	1.706222
209.025240	800.226600	18.760141	-0.040093	1.699687
208.907244	792.379920	18.765146	-0.040066	1.693146
208.783674	784.494149	18.770151	-0.040038	1.686546
208.983618	776.599602	18.775155	-0.040070	1.679956
208.948469	768.743052	18.780160	-0.040059	1.673341
208.738962	760.885288	18.785165	-0.040015	1.666675
208.546440	753.058616	18.790170	-0.039974	1.660010
208.417703	745.200673	18.795175	-0.039945	1.653301
208.453127	737.315748	18.800179	-0.039947	1.646564
208.407977	729.453710	18.805184	-0.039933	1.639808
208.372108	721.585713	18.810189	-0.039922	1.633019
208.529504	713.654366	18.815194	-0.039946	1.626175
208.129139	705.861045	18.820199	-0.039867	1.619344
208.042671	698.014796	18.825203	-0.039846	1.612481
208.062534	690.129660	18.830208	-0.039844	1.605570
208.065651	682.298582	18.835213	-0.039840	1.598675
207.916416	674.481159	18.840218	-0.039807	1.591740
207.702600	666.634297	18.845223	-0.039763	1.584739
207.686869	658.795045	18.850227	-0.039755	1.577742
207.745574	650.924099	18.855232	-0.039761	1.570696
207.628650	643.100442	18.860237	-0.039734	1.563636
207.771916	635.254061	18.865242	-0.039756	1.556561
207.562630	627.415525	18.870247	-0.039712	1.549409
207.562524	619.576853	18.875251	-0.039707	1.542255
207.428586	611.760189	18.880256	-0.039677	1.535068
207.303274	603.937889	18.885261	-0.039649	1.527843
207.176717	596.130640	18.890266	-0.039621	1.520597
207.262797	588.286672	18.895271	-0.039632	1.513315
207.292276	580.453511	18.900275	-0.039632	1.505999
206.947044	572.679179	18.905280	-0.039563	1.498645
207.088169	564.827018	18.910285	-0.039584	1.491256
207.061136	557.017061	18.915290	-0.039575	1.483844
206.814885	549.241630	18.920295	-0.039524	1.476394
206.526352	541.420921	18.925299	-0.039465	1.468856
206.590922	533.577280	18.930304	-0.039472	1.461312
206.554826	525.785519	18.935309	-0.039461	1.453764
206.350377	517.994516	18.940314	-0.039418	1.446150
206.279249	510.204096	18.945319	-0.039400	1.438518
206.437113	502.386030	18.950323	-0.039424	1.430855
206.301762	494.606163	18.955328	-0.039394	1.423141
206.167981	486.841967	18.960333	-0.039364	1.415400
205.997874	479.071024	18.965338	-0.039328	1.407604
205.915149	471.289413	18.970343	-0.039307	1.399769
205.876371	463.511571	18.975347	-0.039295	1.391900
205.716392	455.728713	18.980352	-0.039261	1.383961
205.797202	447.938067	18.985357	-0.039271	1.376009
205.772183	440.166546	18.990362	-0.039261	1.368013
205.741259	432.401475	18.995367	-0.039251	1.359975
205.551305	424.675695	19.000371	-0.039210	1.351903
205.543908	416.906809	19.005376	-0.039204	1.343769
205.296535	409.190310	19.010381	-0.039153	1.335598
205.295036	401.427855	19.015386	-0.039148	1.327372
205.346563	393.672814	19.020391	-0.039153	1.319112
205.247211	385.873539	19.025395	-0.039130	1.310725
205.197115	378.088587	19.030400	-0.039115	1.302308
205.184503	370.365169	19.035405	-0.039108	1.293911
205.009305	362.663722	19.040410	-0.039071	1.285453
204.829184	354.984213	19.045415	-0.039032	1.276962
204.941873	347.243462	19.050419	-0.039048	1.268401
204.769768	339.560429	19.055424	-0.039012	1.259793
204.590342	331.876897	19.060429	-0.038973	1.251123
204.522142	324.185822	19.065434	-0.038956	1.242406
204.454112	316.490810	19.070439	-0.038938	1.233622
204.484527	308.779541	19.075443	-0.038939	1.224776
204.227024	301.131603	19.080448	-0.038887	1.215882
204.149866	293.454617	19.085453	-0.038867	1.206925
204.215066	285.782600	19.090458	-0.038875	1.197935
203.944409	278.146559	19.095463	-0.038819	1.188852
204.150058	270.455868	19.100467	-0.038853	1.179730
204.001067	262.823128	19.105472	-0.038820	1.170535
203.849259	255.198252	19.110477	-0.038787	1.161275
203.813036	247.558921	19.115482	-0.038776	1.151948
203.683170	239.907258	19.120487	-0.038747	1.142509
203.617157	232.298434	19.125491	-0.038730	1.133058
203.501319	224.692447	19.130496	-0.038704	1.123521
203.352711	217.115013	19.135501	-0.038671	1.113931
203.176280	209.537604	19.140506	-0.038634	1.104252
203.105018	201.950188	19.145511	-0.038616	1.094498
203.031998	194.371084	19.150515	-0.038597	1.084666
202.848519	186.831314	19.155520	-0.038558	1.074770
202.747887	179.263238	19.160525	-0.038535	1.064764
202.712980	171.719260	19.165530	-0.038524	1.054711
202.581297	164.182681	19.170535	-0.038494	1.044548
202.553382	156.662403	19.175539	-0.038484	1.034332
202.438132	149.146240	19.180544	-0.038458	1.023999
202.408312	141.645989	19.185549	-0.038448	1.013603
202.273502	134.172131	19.190554	-0.038418	1.003111
201.906134	126.734418	19.195559	-0.038345	0.992502
202.135851	119.191925	19.200563	-0.038383	0.981777
201.906721	111.768316	19.205568	-0.038336	0.970990
201.746457	104.347416	19.210573	-0.038301	0.960103
201.902489	96.895594	19.215578	-0.038326	0.949128
201.628596	89.517920	19.220583	-0.038270	0.938023
201.822211	82.088040	19.225587	-0.038302	0.926829
201.371435	74.793878	19.230592	-0.038213	0.915534
201.036975	67.467712	19.235597	-0.038146	0.904080
201.189435	60.321426	19.240602	-0.038170	0.892898