Thu Mar 11 18:27:16 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.552043	-0.101329	0.000000	-0.000032	0.724600

0.638689	-0.119818	0.005005	-0.000048	0.724594
0.582447	-0.110715	0.010010	-0.000038	0.724593
0.639488	-0.116995	0.015014	-0.000049	0.724601
0.379591	-0.075465	0.020019	-0.000000	0.724592
0.358748	-0.067719	0.025024	0.000003	0.724601
0.351550	-0.070977	0.030029	0.000004	0.724592
0.343080	-0.068345	0.035034	0.000006	0.724595
0.581600	-0.109965	0.040038	-0.000039	0.724597
0.484776	-0.096070	0.045043	-0.000021	0.724591
0.393110	-0.074480	0.050048	-0.000004	0.724602
0.446789	-0.088496	0.055053	-0.000015	0.724593
0.399048	-0.078354	0.060058	-0.000006	0.724597
0.579465	-0.108473	0.065062	-0.000040	0.724602
0.374402	-0.076345	0.070067	-0.000002	0.724593
0.286383	-0.214768	0.075072	0.000014	0.724292
0.448640	-0.257441	0.080077	-0.000016	0.724266
0.548395	-0.278024	0.085082	-0.000035	0.724261
0.539557	-0.273135	0.090086	-0.000034	0.724268
0.495449	-0.268863	0.095091	-0.000026	0.724261
0.480715	-0.262526	0.100096	-0.000023	0.724269
0.269392	-0.293690	0.105101	0.000016	0.724134
0.149704	-0.364783	0.110106	0.000038	0.723954
0.404762	-0.407596	0.115110	-0.000010	0.723959
0.240651	-0.384229	0.120115	0.000021	0.723948
0.447830	-0.416406	0.125120	-0.000018	0.723958
0.508188	-0.464717	0.130125	-0.000030	0.723885
0.483497	-0.588736	0.135130	-0.000025	0.723634
0.345099	-0.562496	0.140134	0.000000	0.723637
0.563377	-0.605175	0.145139	-0.000040	0.723630
0.551014	-0.612764	0.150144	-0.000038	0.723612
0.380053	-0.720566	0.155149	-0.000007	0.723341
0.420949	-0.728677	0.160154	-0.000015	0.723340
0.654915	-0.767022	0.165158	-0.000058	0.723347
0.347801	-0.789719	0.170163	-0.000001	0.723196
0.378352	-0.891381	0.175168	-0.000007	0.723007
0.283214	-0.875191	0.180173	0.000010	0.723006
0.409654	-0.899209	0.185178	-0.000014	0.723004
0.380277	-1.050638	0.190182	-0.000008	0.722697
0.190487	-1.021174	0.195187	0.000027	0.722689
0.250070	-1.026805	0.200192	0.000016	0.722699
0.329342	-1.182285	0.205197	0.000001	0.722422
0.239138	-1.193015	0.210202	0.000017	0.722370
0.200135	-1.183917	0.215206	0.000024	0.722375
0.423017	-1.360295	0.220211	-0.000017	0.722107
0.428742	-1.375973	0.225216	-0.000019	0.722078
0.153708	-1.356599	0.230221	0.000032	0.722021
0.025292	-1.474409	0.235226	0.000056	0.721745
0.132194	-1.491612	0.240230	0.000036	0.721749
0.345990	-1.612170	0.245235	-0.000004	0.721587
0.352827	-1.689107	0.250240	-0.000006	0.721439
0.270677	-1.688091	0.255245	0.000009	0.721413
0.134469	-1.814833	0.260250	0.000035	0.721116
0.392732	-1.857443	0.265254	-0.000014	0.721123
0.161489	-1.908363	0.270259	0.000029	0.720943
0.109296	-1.929336	0.275264	0.000039	0.720884
0.346657	-2.047092	0.280269	-0.000006	0.720735
0.164492	-2.114593	0.285274	0.000028	0.720539
0.011525	-2.121013	0.290278	0.000056	0.720473
0.029919	-2.253208	0.295283	0.000053	0.720220
0.138850	-2.284929	0.300288	0.000032	0.720196
-0.012378	-2.410522	0.305293	0.000060	0.719896
-0.409012	-2.340356	0.310298	0.000134	0.719896
-1.838079	-2.226628	0.315302	0.000400	0.719619
-4.209634	-1.816189	0.320307	0.000841	0.719596
-3.603821	-1.920312	0.325312	0.000728	0.719604
-3.638413	-2.005889	0.330317	0.000734	0.719423
-4.963791	-1.851545	0.335322	0.000980	0.719263
-4.279970	-1.968695	0.340326	0.000853	0.719272
-4.495712	-1.935690	0.345331	0.000893	0.719262
-4.832979	-1.939101	0.350336	0.000955	0.719137
-5.277698	-1.952799	0.355341	0.001038	0.718955
-5.172958	-1.972714	0.360346	0.001018	0.718953
-5.622075	-1.889161	0.365350	0.001101	0.718960
-5.667162	-1.885952	0.370355	0.001110	0.718951
-5.520396	-2.047327	0.375360	0.001082	0.718685
-6.157749	-1.956151	0.380365	0.001201	0.718641
-6.754232	-1.851017	0.385370	0.001311	0.718639
-6.210417	-1.944981	0.390374	0.001210	0.718646
-6.412741	-1.913252	0.395379	0.001247	0.718637
-7.092126	-1.922125	0.400384	0.001374	0.718382
-7.429583	-1.876722	0.405389	0.001436	0.718353
-7.279826	-1.904536	0.410394	0.001408	0.718351
-7.070420	-1.938666	0.415398	0.001369	0.718358
-7.476035	-1.870845	0.420403	0.001444	0.718350
-7.434781	-1.923326	0.425408	0.001436	0.718261
-8.333634	-1.887583	0.430413	0.001603	0.718016
-8.298556	-1.894221	0.435418	0.001596	0.718015
-8.356997	-1.881832	0.440422	0.001607	0.718020
-8.412492	-1.877356	0.445427	0.001617	0.718010
-8.454201	-1.867354	0.450432	0.001625	0.718015
-8.366375	-1.885324	0.455437	0.001608	0.718011
-8.594930	-1.989458	0.460442	0.001650	0.717725
-9.360066	-1.864229	0.465446	0.001793	0.717704
-9.694180	-1.809452	0.470451	0.001855	0.717695
-9.026817	-1.923893	0.475456	0.001730	0.717704
-9.215549	-1.893629	0.480461	0.001765	0.717698
-9.571653	-1.830710	0.485466	0.001831	0.717698
-9.110802	-1.954332	0.490470	0.001745	0.717616
-9.971927	-1.925303	0.495475	0.001905	0.717370
-10.042922	-1.908667	0.500480	0.001918	0.717379
-10.411199	-1.847170	0.505485	0.001986	0.717371
-10.322381	-1.861407	0.510490	0.001970	0.717375
-9.987123	-1.920013	0.515494	0.001907	0.717377
-10.190173	-1.886921	0.520499	0.001945	0.717372
-10.306583	-1.955257	0.525504	0.001966	0.717196
-10.953987	-1.899517	0.530509	0.002086	0.717079
-11.008571	-1.888844	0.535514	0.002096	0.717081
-10.825248	-1.921099	0.540518	0.002062	0.717082
-11.100159	-1.875085	0.545523	0.002113	0.717077
-11.047244	-1.882218	0.550528	0.002103	0.717082
-11.334453	-1.832041	0.555533	0.002156	0.717080
-11.451185	-1.948953	0.560538	0.002177	0.716808
-11.856774	-1.903836	0.565542	0.002253	0.716755
-12.441833	-1.804546	0.570547	0.002361	0.716746
-11.804649	-1.914887	0.575552	0.002242	0.716753
-11.801589	-1.916650	0.580557	0.002242	0.716751
-12.255539	-1.837165	0.585562	0.002326	0.716748
-12.211668	-1.841782	0.590566	0.002317	0.716755
-12.313287	-1.901593	0.595571	0.002336	0.716601
-12.973657	-1.862250	0.600576	0.002459	0.716447
-12.840245	-1.888770	0.605581	0.002434	0.716442
-12.855872	-1.888505	0.610586	0.002436	0.716437
-12.719346	-1.909509	0.615590	0.002411	0.716444
-12.892643	-1.883996	0.620595	0.002443	0.716434
-13.016041	-1.857360	0.625600	0.002466	0.716444
-12.968308	-1.941927	0.630605	0.002456	0.716294
-14.020666	-1.840994	0.635610	0.002652	0.716123
-13.707486	-1.892444	0.640614	0.002594	0.716132
-13.942614	-1.856269	0.645619	0.002637	0.716121
-14.034905	-1.837657	0.650624	0.002654	0.716126
-13.919714	-1.859670	0.655629	0.002632	0.716123
-13.812364	-1.878474	0.660634	0.002612	0.716124
-13.576973	-1.947744	0.665638	0.002568	0.716071
-14.875239	-1.816956	0.670643	0.002810	0.715872
-14.758378	-1.832531	0.675648	0.002788	0.715883
-14.646362	-1.854924	0.680653	0.002766	0.715879
-14.796216	-1.830194	0.685658	0.002794	0.715875
-14.569751	-1.867067	0.690662	0.002752	0.715882
-14.795161	-1.833131	0.695667	0.002793	0.715871
-14.509972	-1.893541	0.700672	0.002740	0.715852
-15.467661	-1.879291	0.705677	0.002918	0.715543
-15.776785	-1.825518	0.710682	0.002975	0.715540
-15.452869	-1.880107	0.715686	0.002915	0.715547
-15.533440	-1.869923	0.720691	0.002930	0.715539
-15.730215	-1.832110	0.725696	0.002966	0.715545
-15.746158	-1.829345	0.730701	0.002969	0.715546
-15.746525	-1.832504	0.735706	0.002969	0.715540
-15.907666	-1.923248	0.740710	0.002998	0.715303
-16.808041	-1.804792	0.745715	0.003166	0.715220
-16.659569	-1.826556	0.750720	0.003138	0.715230
-16.459089	-1.863605	0.755725	0.003100	0.715228
-16.683993	-1.824283	0.760730	0.003142	0.715227
-16.180178	-1.909350	0.765734	0.003048	0.715237
-16.543397	-1.849401	0.770739	0.003115	0.715228
-16.914285	-1.875583	0.775744	0.003184	0.715045
-17.580902	-1.825379	0.780749	0.003308	0.714910
-17.646508	-1.816755	0.785754	0.003320	0.714904
-17.632621	-1.813995	0.790758	0.003317	0.714915
-17.972118	-1.758387	0.795763	0.003380	0.714906
-17.433791	-1.851770	0.800768	0.003280	0.714911
-17.749231	-1.797301	0.805773	0.003338	0.714908
-18.006400	-1.752859	0.810778	0.003386	0.714906
-17.427845	-1.949084	0.815782	0.003278	0.714721
-18.654469	-1.788896	0.820787	0.003506	0.714606
-18.535680	-1.808798	0.825792	0.003484	0.714609
-18.173454	-1.873169	0.830797	0.003416	0.714610
-18.692597	-1.783076	0.835802	0.003512	0.714606
-18.457089	-1.820273	0.840806	0.003468	0.714615
-18.672807	-1.787774	0.845811	0.003508	0.714604
-18.601606	-1.855527	0.850816	0.003495	0.714495
-19.610798	-1.786001	0.855821	0.003682	0.714277
-19.623775	-1.785886	0.860826	0.003684	0.714273
-19.499133	-1.804867	0.865830	0.003661	0.714280
-19.670393	-1.778832	0.870835	0.003693	0.714271
-19.979440	-1.720625	0.875840	0.003750	0.714278
-19.588535	-1.791248	0.880845	0.003677	0.714276
-19.493617	-1.810002	0.885850	0.003659	0.714273
-19.573715	-1.845822	0.890854	0.003674	0.714174
-20.654668	-1.758546	0.895859	0.003875	0.713965
-19.864114	-1.895306	0.900864	0.003727	0.713974
-20.429938	-1.796771	0.905869	0.003832	0.713970
-20.752950	-1.742362	0.910874	0.003892	0.713964
-20.034484	-1.865139	0.915878	0.003758	0.713975
-20.195569	-1.842838	0.920883	0.003788	0.713963
-20.492879	-1.817435	0.925888	0.003843	0.713908
-21.230808	-1.814941	0.930893	0.003980	0.713653
-21.328165	-1.802185	0.935898	0.003998	0.713644
-21.458661	-1.772847	0.940902	0.004022	0.713656
-21.659864	-1.743473	0.945907	0.004059	0.713644
-21.372575	-1.791123	0.950912	0.004006	0.713652
-21.511604	-1.766977	0.955917	0.004031	0.713651
-21.607220	-1.751823	0.960922	0.004049	0.713647
-21.241674	-1.867389	0.965926	0.003981	0.713548
-22.303798	-1.774181	0.970931	0.004178	0.713357
-22.536317	-1.730827	0.975936	0.004221	0.713361
-22.281219	-1.778512	0.980941	0.004173	0.713357
-22.128101	-1.807399	0.985946	0.004145	0.713355
-22.240462	-1.784551	0.990950	0.004165	0.713361
-22.797363	-1.689719	0.995955	0.004269	0.713353
-22.075599	-1.813644	1.000960	0.004134	0.713362
-22.383349	-1.914713	1.005965	0.004191	0.713053
-23.532983	-1.727328	1.010970	0.004405	0.713018
-23.333140	-1.758422	1.015974	0.004368	0.713028
-22.733115	-1.868623	1.020979	0.004256	0.713022
-23.259607	-1.773440	1.025984	0.004353	0.713025
-23.545151	-1.723894	1.030989	0.004406	0.713023
-23.210647	-1.785374	1.035994	0.004344	0.713019
-23.140284	-1.895278	1.040998	0.004331	0.712826
-24.307323	-1.748495	1.046003	0.004548	0.712705
-23.781522	-1.839788	1.051008	0.004449	0.712710
-23.952043	-1.810382	1.056013	0.004481	0.712709
-24.399543	-1.733310	1.061018	0.004564	0.712704
-23.778550	-1.840623	1.066022	0.004448	0.712711
-23.807733	-1.840673	1.071027	0.004453	0.712701
-24.483659	-1.840484	1.076032	0.004579	0.712462
-24.963414	-1.794732	1.081037	0.004668	0.712383
-24.952000	-1.798252	1.086042	0.004666	0.712381
-24.896482	-1.804380	1.091046	0.004655	0.712389
-25.488979	-1.705270	1.096051	0.004765	0.712376
-25.201017	-1.753247	1.101056	0.004711	0.712383
-24.588705	-1.861564	1.106061	0.004597	0.712385
-25.257298	-1.797948	1.111066	0.004721	0.712275
-26.180131	-1.724545	1.116070	0.004893	0.712094
-25.692097	-1.816164	1.121075	0.004802	0.712085
-25.939649	-1.769701	1.126080	0.004848	0.712091
-25.889412	-1.779943	1.131085	0.004838	0.712089
-25.723087	-1.811575	1.136090	0.004807	0.712085
-25.802960	-1.793228	1.141094	0.004821	0.712094
-25.871130	-1.796627	1.146099	0.004834	0.712063
-26.366228	-1.860134	1.151104	0.004926	0.711761
-26.667808	-1.807998	1.156109	0.004982	0.711758
-27.031976	-1.745179	1.161114	0.005049	0.711755
-26.540787	-1.829022	1.166118	0.004958	0.711763
-26.648419	-1.815439	1.171123	0.004977	0.711752
-27.071425	-1.736029	1.176128	0.005056	0.711760
-26.794809	-1.786452	1.181133	0.005004	0.711759
-27.008600	-1.894499	1.186138	0.005044	0.711468
-27.480131	-1.815403	1.191142	0.005131	0.711458
-28.001116	-1.727260	1.196147	0.005228	0.711449
-27.704327	-1.778539	1.201152	0.005173	0.711453
-27.365406	-1.838892	1.206157	0.005109	0.711454
-27.805902	-1.762548	1.211162	0.005191	0.711450
-27.873955	-1.744393	1.216166	0.005203	0.711462
-28.079953	-1.834284	1.221171	0.005242	0.711210
-28.687059	-1.761221	1.226176	0.005354	0.711141
-28.631034	-1.773862	1.231181	0.005344	0.711136
-28.385430	-1.818565	1.236186	0.005298	0.711134
-28.416325	-1.808481	1.241190	0.005303	0.711144
-28.539628	-1.792843	1.246195	0.005326	0.711132
-28.757121	-1.750016	1.251200	0.005366	0.711140
-28.898843	-1.801331	1.256205	0.005392	0.710988
-29.593980	-1.738841	1.261210	0.005521	0.710866
-29.324152	-1.783756	1.266214	0.005471	0.710873
-29.241087	-1.801801	1.271219	0.005455	0.710867
-29.311262	-1.788355	1.276224	0.005468	0.710869
-29.449281	-1.763875	1.281229	0.005494	0.710869
-29.584551	-1.742153	1.286234	0.005518	0.710865
-29.292872	-1.885679	1.291238	0.005464	0.710683
-30.531206	-1.743747	1.296243	0.005694	0.710526
-30.659767	-1.718959	1.301248	0.005718	0.710530
-30.184957	-1.804119	1.306253	0.005629	0.710529
-30.588868	-1.733896	1.311258	0.005704	0.710526
-30.532160	-1.740600	1.316262	0.005693	0.710534
-30.527791	-1.745714	1.321267	0.005692	0.710525
-30.419103	-1.779148	1.326272	0.005672	0.710498
-31.263228	-1.769707	1.331277	0.005829	0.710217
-31.376467	-1.751595	1.336282	0.005850	0.710213
-31.388230	-1.744458	1.341286	0.005852	0.710223
-31.252339	-1.774884	1.346291	0.005826	0.710211
-31.266252	-1.768340	1.351296	0.005828	0.710220
-31.342049	-1.755104	1.356301	0.005842	0.710220
-31.286721	-1.767892	1.361306	0.005832	0.710215
-31.569396	-1.838964	1.366310	0.005884	0.709972
-32.447544	-1.723302	1.371315	0.006047	0.709891
-32.115580	-1.781329	1.376320	0.005985	0.709894
-32.267427	-1.755320	1.381325	0.006013	0.709892
-32.611899	-1.696583	1.386330	0.006077	0.709887
-31.885237	-1.822257	1.391334	0.005942	0.709896
-31.983563	-1.808441	1.396339	0.005960	0.709889
-32.464389	-1.809523	1.401344	0.006049	0.709716
-33.127329	-1.751513	1.406349	0.006172	0.709596
-32.984988	-1.781640	1.411354	0.006146	0.709587
-33.106206	-1.753675	1.416358	0.006168	0.709600
-33.473010	-1.692750	1.421363	0.006236	0.709591
-32.895438	-1.796307	1.426368	0.006128	0.709591
-32.819142	-1.808849	1.431373	0.006114	0.709593
-33.425542	-1.776393	1.436378	0.006226	0.709442
-34.017038	-1.758159	1.441382	0.006336	0.709268
-33.828077	-1.797685	1.446387	0.006301	0.709257
-34.228365	-1.724900	1.451392	0.006375	0.709261
-34.019001	-1.761861	1.456397	0.006336	0.709262
-33.792182	-1.805521	1.461402	0.006293	0.709256
-33.802353	-1.797778	1.466406	0.006295	0.709268
-34.009497	-1.820451	1.471411	0.006333	0.709149
-34.946204	-1.750984	1.476416	0.006508	0.708955
-34.826424	-1.770693	1.481421	0.006485	0.708958
-35.096931	-1.727198	1.486426	0.006535	0.708949
-34.639033	-1.802685	1.491430	0.006450	0.708962
-34.872729	-1.768167	1.496435	0.006493	0.708948
-35.262992	-1.694011	1.501440	0.006565	0.708958
-34.880919	-1.775749	1.506445	0.006494	0.708931
-35.322025	-1.846057	1.511450	0.006576	0.708633
-35.902274	-1.737300	1.516454	0.006684	0.708645
-36.332470	-1.664911	1.521459	0.006763	0.708636
-35.722273	-1.771600	1.526464	0.006650	0.708641
-35.673617	-1.782063	1.531469	0.006640	0.708638
-36.451204	-1.647370	1.536474	0.006785	0.708631
-36.098778	-1.705700	1.541478	0.006719	0.708640
-35.978785	-1.786037	1.546483	0.006696	0.708522
-36.844416	-1.720610	1.551488	0.006857	0.708345
-36.511638	-1.778986	1.556493	0.006795	0.708347
-36.804185	-1.728986	1.561498	0.006849	0.708343
-36.879805	-1.711145	1.566502	0.006863	0.708353
-36.780162	-1.733149	1.571507	0.006844	0.708345
-36.789311	-1.731166	1.576512	0.006846	0.708346
-36.669187	-1.793626	1.581517	0.006823	0.708264
-37.678751	-1.742337	1.586522	0.007011	0.708007
-37.260915	-1.813345	1.591526	0.006933	0.708014
-37.726195	-1.737032	1.596531	0.007019	0.708001
-37.462119	-1.779584	1.601536	0.006970	0.708011
-37.632209	-1.748838	1.606541	0.007001	0.708012
-37.775224	-1.726305	1.611546	0.007028	0.708007
-37.669504	-1.784699	1.616550	0.007008	0.707928
-38.731664	-1.712020	1.621555	0.007205	0.707694
-38.343510	-1.777624	1.626560	0.007133	0.707702
-38.184743	-1.808685	1.631565	0.007103	0.707697
-38.614901	-1.735009	1.636570	0.007183	0.707691
-38.825008	-1.692344	1.641574	0.007222	0.707702
-38.550237	-1.745910	1.646579	0.007170	0.707693
-38.573491	-1.739118	1.651584	0.007174	0.707699
-38.989561	-1.822440	1.656589	0.007252	0.707384
-39.206977	-1.789248	1.661594	0.007292	0.707373
-39.280706	-1.771049	1.666598	0.007305	0.707384
-39.280854	-1.776934	1.671603	0.007305	0.707372
-39.453012	-1.744924	1.676608	0.007337	0.707375
-39.305680	-1.771262	1.681613	0.007309	0.707376
-39.462670	-1.766031	1.686618	0.007338	0.707331
-40.113388	-1.772996	1.691622	0.007459	0.707084
-40.089588	-1.782408	1.696627	0.007455	0.707074
-40.483129	-1.708916	1.701632	0.007528	0.707081
-40.525056	-1.702064	1.706637	0.007535	0.707081
-40.354350	-1.735368	1.711642	0.007503	0.707075
-40.102120	-1.775778	1.716646	0.007456	0.707085
-40.624283	-1.687135	1.721651	0.007553	0.707077
-40.632363	-1.818433	1.726656	0.007554	0.706810
-40.873902	-1.805495	1.731661	0.007599	0.706750
-41.201761	-1.749811	1.736666	0.007660	0.706745
-41.187972	-1.748266	1.741670	0.007657	0.706754
-41.045459	-1.778721	1.746675	0.007630	0.706744
-40.854247	-1.810900	1.751680	0.007594	0.706748
-40.894668	-1.829185	1.756685	0.007602	0.706698
-41.935104	-1.774717	1.761690	0.007795	0.706435
-41.715497	-1.809513	1.766694	0.007754	0.706444
-42.234552	-1.720949	1.771699	0.007850	0.706437
-42.205196	-1.723657	1.776704	0.007845	0.706442
-41.754185	-1.802537	1.781709	0.007760	0.706446
-42.301404	-1.708138	1.786714	0.007862	0.706440
-42.267716	-1.710647	1.791718	0.007856	0.706447
-42.357306	-1.847248	1.796723	0.007872	0.706141
-43.187760	-1.705461	1.801728	0.008026	0.706129
-43.277327	-1.690504	1.806733	0.008043	0.706128
-42.774580	-1.783773	1.811738	0.007949	0.706121
-42.661790	-1.799142	1.816742	0.007928	0.706131
-43.177268	-1.712765	1.821747	0.008023	0.706120
-43.257241	-1.695597	1.826752	0.008038	0.706126
-42.906012	-1.837551	1.831757	0.007973	0.705967
-43.895868	-1.716944	1.836762	0.008156	0.705856
-43.530557	-1.777719	1.841766	0.008088	0.705865
-43.431903	-1.800040	1.846771	0.008070	0.705856
-43.619996	-1.764181	1.851776	0.008104	0.705861
-43.498720	-1.784597	1.856781	0.008082	0.705864
-44.082818	-1.693279	1.861786	0.008190	0.705838
-44.575842	-1.760848	1.866790	0.008282	0.705526
-44.483660	-1.779880	1.871795	0.008264	0.705521
-44.999545	-1.687526	1.876800	0.008360	0.705523
-44.288870	-1.814217	1.881805	0.008228	0.705523
-44.662525	-1.749817	1.886810	0.008297	0.705519
-44.925401	-1.699076	1.891814	0.008346	0.705527
-44.661091	-1.748676	1.896819	0.008296	0.705523
-45.063962	-1.817510	1.901824	0.008371	0.705240
-45.730027	-1.712533	1.906829	0.008495	0.705213
-45.971647	-1.672018	1.911834	0.008539	0.705208
-45.101321	-1.823490	1.916838	0.008377	0.705216
-45.462834	-1.762260	1.921843	0.008444	0.705210
-45.947204	-1.675251	1.926848	0.008534	0.705212
-45.499454	-1.756430	1.931853	0.008450	0.705210
-45.720180	-1.840501	1.936858	0.008491	0.704962
-46.609399	-1.714915	1.941862	0.008657	0.704896
-46.299145	-1.776272	1.946867	0.008599	0.704884
-46.083029	-1.813947	1.951872	0.008558	0.704886
-46.354106	-1.764846	1.956877	0.008608	0.704888
-46.657594	-1.714035	1.961882	0.008665	0.704882
-46.535007	-1.732751	1.966886	0.008642	0.704889
-46.961242	-1.780550	1.971891	0.008721	0.704640
-47.442820	-1.720145	1.976896	0.008810	0.704589
-46.959342	-1.807695	1.981901	0.008720	0.704587
-46.991904	-1.804214	1.986906	0.008726	0.704583
-47.451012	-1.717910	1.991910	0.008811	0.704592
-47.262528	-1.756781	1.996915	0.008776	0.704582
-47.421735	-1.788522	2.001920	0.008805	0.704461

-48.223266	-1.747240	2.011917	0.008954	0.704257
-48.359564	-1.724529	2.021914	0.008979	0.704255
-48.042996	-1.781316	2.031910	0.008919	0.704255
-48.419987	-1.713600	2.041907	0.008989	0.704257
-48.293083	-1.737310	2.051904	0.008965	0.704256
-48.192151	-1.756351	2.061901	0.008946	0.704255
-48.358241	-1.728212	2.071898	0.008976	0.704253
-48.219451	-1.752607	2.081894	0.008950	0.704255
-48.441945	-1.710807	2.091891	0.008991	0.704260
-47.533653	-1.761311	2.101888	0.008821	0.704485
-47.366551	-1.739252	2.111885	0.008789	0.704591
-47.394264	-1.736560	2.121882	0.008794	0.704587
-47.374385	-1.739871	2.131878	0.008790	0.704589
-47.238048	-1.762159	2.141875	0.008764	0.704594
-47.227557	-1.764378	2.151872	0.008762	0.704594
-47.424881	-1.731254	2.161869	0.008798	0.704591
-46.680740	-1.725043	2.171866	0.008659	0.704871
-46.526384	-1.744955	2.181862	0.008630	0.704888
-46.568518	-1.736512	2.191859	0.008637	0.704890
-46.471998	-1.756124	2.201856	0.008618	0.704886
-46.303131	-1.687504	2.211853	0.008586	0.705086
-45.620039	-1.749426	2.221850	0.008459	0.705208
-45.652812	-1.742689	2.231846	0.008464	0.705210
-45.445780	-1.780140	2.241843	0.008425	0.705210
-45.034916	-1.760748	2.251840	0.008348	0.705398
-44.608356	-1.774577	2.261837	0.008269	0.705524
-44.721341	-1.756609	2.271834	0.008289	0.705520
-44.820017	-1.739211	2.281830	0.008307	0.705521
-44.287769	-1.725718	2.291827	0.008207	0.705740
-43.786166	-1.753862	2.301824	0.008114	0.705864
-43.922165	-1.732415	2.311821	0.008138	0.705859
-43.490294	-1.810721	2.321818	0.008057	0.705858
-43.219976	-1.748380	2.331814	0.008007	0.706081
-43.124438	-1.742941	2.341811	0.007988	0.706127
-42.995022	-1.766515	2.351808	0.007964	0.706127
-43.019813	-1.699426	2.361805	0.007968	0.706254
-42.184975	-1.755150	2.371802	0.007812	0.706442
-42.217402	-1.751040	2.381798	0.007818	0.706439
-42.060678	-1.778586	2.391795	0.007788	0.706441
-41.436610	-1.747186	2.401792	0.007671	0.706729
-41.498709	-1.727010	2.411789	0.007682	0.706748
-41.250690	-1.771723	2.421786	0.007636	0.706748
-41.170279	-1.707957	2.431782	0.007620	0.706906
-40.269207	-1.783059	2.441779	0.007452	0.707078
-40.504754	-1.740564	2.451776	0.007495	0.707080
-40.419162	-1.753561	2.461773	0.007479	0.707086
-39.881747	-1.708326	2.471770	0.007378	0.707370
-39.556835	-1.766588	2.481766	0.007317	0.707370
-39.307274	-1.809744	2.491763	0.007270	0.707373
-39.223359	-1.737296	2.501760	0.007254	0.707550
-38.725751	-1.753681	2.511757	0.007161	0.707696
-38.678568	-1.761815	2.521754	0.007152	0.707697
-38.838348	-1.718994	2.531750	0.007181	0.707727
-37.879399	-1.748716	2.541747	0.007002	0.708011
-37.893037	-1.746672	2.551744	0.007004	0.708011
-37.788563	-1.765913	2.561741	0.006984	0.708011
-37.426446	-1.718637	2.571738	0.006916	0.708236
-36.996236	-1.741300	2.581734	0.006836	0.708345
-37.011750	-1.737986	2.591731	0.006838	0.708347
-36.902229	-1.727588	2.601728	0.006817	0.708408
-36.230236	-1.734420	2.611725	0.006692	0.708635
-35.892314	-1.795151	2.621722	0.006628	0.708635
-36.246479	-1.732493	2.631718	0.006694	0.708635
-35.557456	-1.737090	2.641715	0.006565	0.708873
-35.217905	-1.757516	2.651712	0.006501	0.708954
-35.159979	-1.769437	2.661709	0.006490	0.708952
-35.449203	-1.679824	2.671706	0.006543	0.709029
-34.356386	-1.760454	2.681702	0.006339	0.709258
-34.377348	-1.756753	2.691699	0.006343	0.709259
-34.571032	-1.720864	2.701696	0.006378	0.709263
-33.622891	-1.740387	2.711693	0.006201	0.709563
-33.530497	-1.742510	2.721690	0.006184	0.709592
-33.367276	-1.770579	2.731686	0.006153	0.709595
-33.430363	-1.707947	2.741683	0.006164	0.709699
-32.633233	-1.753271	2.751680	0.006015	0.709893
-32.722489	-1.738650	2.761677	0.006031	0.709892
-32.854483	-1.715395	2.771674	0.006055	0.709892
-31.994891	-1.707690	2.781670	0.005895	0.710215
-31.801757	-1.739288	2.791667	0.005858	0.710221
-31.734768	-1.751104	2.801664	0.005845	0.710222
-31.319935	-1.746956	2.811661	0.005768	0.710379
-31.053930	-1.717833	2.821658	0.005718	0.710533
-31.048061	-1.718521	2.831654	0.005716	0.710535
-30.977215	-1.707430	2.841651	0.005702	0.710583
-29.912924	-1.751807	2.851648	0.005504	0.710874
-30.018374	-1.735320	2.861645	0.005523	0.710870
-30.199201	-1.704187	2.871642	0.005556	0.710869
-29.516188	-1.753624	2.881638	0.005428	0.711014
-29.208162	-1.746679	2.891635	0.005370	0.711139
-29.172860	-1.753082	2.901632	0.005363	0.711139
-29.170141	-1.745846	2.911629	0.005362	0.711156
-28.770523	-1.668319	2.921626	0.005287	0.711453
-28.267663	-1.757646	2.931622	0.005193	0.711455
-28.319573	-1.749840	2.941619	0.005203	0.711453
-27.803479	-1.734469	2.951616	0.005106	0.711668
-27.572475	-1.729926	2.961613	0.005062	0.711760
-27.438451	-1.755565	2.971610	0.005037	0.711757
-27.513730	-1.697889	2.981606	0.005051	0.711847
-26.686031	-1.724057	2.991603	0.004896	0.712089
-26.396865	-1.776399	3.001600	0.004842	0.712089
-26.474091	-1.762907	3.011597	0.004856	0.712089
-26.169695	-1.706140	3.021594	0.004798	0.712311
-25.655751	-1.763343	3.031590	0.004702	0.712380
-25.738826	-1.746298	3.041587	0.004717	0.712386
-25.382436	-1.779505	3.051584	0.004650	0.712447
-24.999359	-1.716718	3.061581	0.004579	0.712709
-24.460598	-1.814395	3.071578	0.004478	0.712707
-24.897122	-1.737001	3.081574	0.004559	0.712707
-24.522687	-1.700188	3.091571	0.004488	0.712914
-23.930710	-1.750055	3.101568	0.004378	0.713025
-24.203856	-1.701695	3.111565	0.004428	0.713026
-23.943652	-1.693067	3.121562	0.004379	0.713136
-22.955000	-1.758825	3.131558	0.004194	0.713357
-23.034095	-1.744412	3.141555	0.004209	0.713358
-22.820035	-1.781247	3.151552	0.004168	0.713362
-22.884785	-1.665452	3.161549	0.004180	0.713570
-22.236809	-1.742533	3.171546	0.004059	0.713647
-22.493295	-1.695217	3.181542	0.004106	0.713651
-21.898739	-1.734194	3.191539	0.003995	0.713785
-21.156937	-1.774105	3.201536	0.003856	0.713970
-21.540943	-1.706744	3.211533	0.003927	0.713968
-21.260715	-1.758000	3.221530	0.003875	0.713967
-20.486248	-1.757089	3.231526	0.003730	0.714244
-20.512809	-1.734724	3.241523	0.003734	0.714280
-20.125425	-1.805384	3.251520	0.003662	0.714277
-20.566349	-1.686021	3.261517	0.003743	0.714359
-19.467970	-1.756904	3.271514	0.003538	0.714608
-19.666489	-1.721805	3.281510	0.003575	0.714608
-19.344861	-1.779057	3.291507	0.003515	0.714609
-19.000989	-1.734923	3.301504	0.003450	0.714819
-18.724574	-1.738049	3.311501	0.003398	0.714912
-18.654337	-1.753389	3.321498	0.003384	0.714907
-18.598138	-1.734054	3.331494	0.003374	0.714966
-17.767192	-1.749294	3.341491	0.003218	0.715231
-17.546372	-1.789451	3.351488	0.003177	0.715230
-17.866643	-1.732742	3.361485	0.003236	0.715230
-17.264687	-1.741895	3.371482	0.003123	0.715426
-17.026873	-1.723360	3.381478	0.003078	0.715547
-16.658967	-1.789009	3.391475	0.003010	0.715548
-16.689836	-1.784132	3.401472	0.003015	0.715548
-16.135714	-1.724267	3.411469	0.002911	0.715863
-15.683583	-1.795888	3.421466	0.002826	0.715882
-15.811166	-1.774020	3.431462	0.002850	0.715881
-15.715034	-1.772600	3.441459	0.002831	0.715919
-14.946662	-1.801904	3.451456	0.002688	0.716133
-14.909098	-1.809099	3.461453	0.002680	0.716133
-14.958643	-1.799870	3.471450	0.002689	0.716134
-14.674403	-1.768625	3.481446	0.002636	0.716297
-13.853173	-1.837988	3.491443	0.002482	0.716451
-14.290737	-1.759325	3.501440	0.002563	0.716453
-14.159393	-1.777699	3.511437	0.002538	0.716464
-13.214526	-1.799142	3.521434	0.002362	0.716755
-13.234466	-1.797516	3.531430	0.002365	0.716753
-13.144561	-1.812849	3.541427	0.002348	0.716755
-13.072563	-1.744669	3.551424	0.002334	0.716916
-12.180365	-1.818934	3.561421	0.002167	0.717084
-12.344143	-1.792161	3.571418	0.002197	0.717081
-12.292861	-1.802194	3.581414	0.002187	0.717080
-11.465739	-1.810942	3.591411	0.002033	0.717355
-11.461859	-1.799411	3.601408	0.002032	0.717380
-11.350734	-1.820301	3.611405	0.002011	0.717379
-11.399693	-1.756868	3.621402	0.002019	0.717488
-10.697476	-1.775271	3.631398	0.001888	0.717700
-10.512100	-1.808082	3.641395	0.001853	0.717701
-10.444000	-1.819727	3.651392	0.001840	0.717703
-9.755664	-1.812680	3.661389	0.001711	0.717960
-9.851052	-1.770284	3.671386	0.001728	0.718011
-9.583902	-1.817856	3.681382	0.001678	0.718012
-9.543915	-1.776426	3.691379	0.001670	0.718109
-8.676816	-1.807589	3.701376	0.001508	0.718353
-8.476504	-1.843572	3.711373	0.001470	0.718353
-8.627832	-1.818746	3.721370	0.001498	0.718350
-8.472414	-1.772120	3.731366	0.001469	0.718498
-7.642240	-1.848149	3.741363	0.001314	0.718640
-7.856416	-1.809874	3.751360	0.001353	0.718642
-7.714844	-1.834959	3.761357	0.001326	0.718643
-7.098916	-1.794271	3.771354	0.001211	0.718940
-6.810335	-1.838882	3.781350	0.001157	0.718955
-6.850266	-1.829501	3.791347	0.001164	0.718960
-6.787630	-1.792155	3.801344	0.001152	0.719057
-5.751703	-1.869532	3.811341	0.000958	0.719269
-5.878698	-1.847300	3.821338	0.000981	0.719269
-5.936801	-1.838130	3.831334	0.000992	0.719268
-5.382769	-1.839519	3.841331	0.000888	0.719460
-4.965679	-1.841711	3.851328	0.000810	0.719603
-4.711679	-1.887569	3.861325	0.000762	0.719603
-4.990302	-1.839325	3.871322	0.000814	0.719601
-4.216736	-1.865244	3.881318	0.000669	0.719823
-4.247440	-1.820733	3.891315	0.000674	0.719900
-4.180232	-1.832889	3.901312	0.000661	0.719901
-3.984917	-1.835686	3.911309	0.000624	0.719965
-3.211146	-1.842530	3.921306	0.000480	0.720224
-3.189698	-1.845901	3.931302	0.000475	0.720226
-3.009958	-1.879287	3.941299	0.000441	0.720224
-3.027781	-1.792352	3.951296	0.000444	0.720390
-2.396464	-1.828143	3.961293	0.000326	0.720541
-2.510502	-1.808974	3.971290	0.000347	0.720540
-2.531464	-1.763894	3.981286	0.000350	0.720622
-2.067652	-1.717755	3.991283	0.000263	0.720877
-1.905799	-1.745571	4.001280	0.000233	0.720879
-1.884493	-1.718605	4.011277	0.000228	0.720941
-1.674801	-1.665422	4.021274	0.000189	0.721120
-1.495841	-1.696800	4.031270	0.000155	0.721122
-1.487311	-1.602605	4.041267	0.000153	0.721311
-1.321511	-1.567201	4.051264	0.000122	0.721439
-1.510200	-1.489418	4.061261	0.000156	0.721527
-1.182244	-1.438286	4.071258	0.000095	0.721743
-1.258056	-1.391323	4.081254	0.000108	0.721810
-0.793436	-1.341324	4.091251	0.000021	0.722072
-0.875850	-1.291260	4.101248	0.000036	0.722142
-0.639135	-1.217535	4.111245	-0.000009	0.722370
-0.786595	-1.131589	4.121242	0.000018	0.722489
-0.643785	-1.054109	4.131238	-0.000009	0.722691
-0.477154	-0.976340	4.141235	-0.000040	0.722903
-0.422036	-0.924944	4.151232	-0.000051	0.723024
-0.477142	-0.753636	4.161229	-0.000042	0.723342
-0.442160	-0.675495	4.171226	-0.000049	0.723508
-0.259279	-0.622628	4.181222	-0.000083	0.723676
-0.223788	-0.489167	4.191219	-0.000090	0.723951
-0.327491	-0.347512	4.201216	-0.000072	0.724193
-0.439902	-0.203748	4.211213	-0.000051	0.724437
-0.489070	-0.060579	4.221210	-0.000043	0.724700
-0.228090	0.018556	4.231206	-0.000092	0.724947
0.000000	0.172075	4.241203	-0.000135	0.725328

-0.165084	0.812028	4.246208	-0.000105	0.726521
-0.012024	2.062681	4.251213	-0.000134	0.729011
0.137489	3.900232	4.256218	-0.000164	0.732629
0.356431	6.278495	4.261222	-0.000206	0.737294
0.757259	9.142191	4.266227	-0.000283	0.742918
0.733071	12.556902	4.271232	-0.000281	0.749400
1.075507	16.363352	4.276237	-0.000347	0.756683
1.531226	20.540941	4.281242	-0.000435	0.764623
1.939467	25.150757	4.286246	-0.000514	0.773258
2.043768	30.168497	4.291251	-0.000537	0.782440
2.724472	35.427647	4.296256	-0.000668	0.792130
3.078101	41.065339	4.301261	-0.000738	0.802270
3.208890	47.044422	4.306266	-0.000766	0.812810
3.713096	53.235438	4.311270	-0.000864	0.823694
4.426731	59.680029	4.316275	-0.001002	0.834929
4.927131	66.364266	4.321280	-0.001099	0.846353
5.315292	73.304763	4.326285	-0.001176	0.858015
6.050890	80.386870	4.331290	-0.001318	0.869852
6.712515	87.673529	4.336294	-0.001446	0.881837
7.044409	95.192701	4.341299	-0.001513	0.893938
7.655170	102.812523	4.346304	-0.001632	0.906111
8.198878	110.601938	4.351309	-0.001739	0.918366
9.054359	118.425224	4.356314	-0.001903	0.930595
10.249503	126.320384	4.361318	-0.002131	0.942861
11.863008	134.279709	4.366323	-0.002437	0.955173
12.855719	142.427006	4.371328	-0.002628	0.967444
13.295880	150.779206	4.376333	-0.002715	0.979718
13.667535	159.212165	4.381338	-0.002790	0.991939
14.194307	167.648685	4.386342	-0.002894	1.004053
15.073140	176.071966	4.391347	-0.003063	1.016089
16.016385	184.511079	4.396352	-0.003245	1.028021
16.742103	193.055583	4.401357	-0.003386	1.039909
17.167338	201.663207	4.406362	-0.003471	1.051676
17.918836	210.244086	4.411366	-0.003617	1.063352
18.753964	218.851396	4.416371	-0.003778	1.074955
19.249265	227.490314	4.421376	-0.003876	1.086398
19.836634	236.148735	4.426381	-0.003991	1.097768
20.975425	244.704198	4.431386	-0.004209	1.109010
21.477718	253.381527	4.436390	-0.004309	1.120154
22.211188	262.012908	4.441395	-0.004451	1.131181
22.941697	270.628635	4.446400	-0.004593	1.142081
23.762337	279.284823	4.451405	-0.004752	1.152946
24.229125	287.936422	4.456410	-0.004844	1.163629
25.012973	296.527255	4.461414	-0.004996	1.174208
25.986131	305.085564	4.466419	-0.005183	1.184691
26.518387	313.713492	4.471424	-0.005288	1.195075
26.767977	322.368319	4.476429	-0.005340	1.205345
27.210824	330.974932	4.481434	-0.005429	1.215510
27.903805	339.520056	4.486438	-0.005564	1.225568
28.692601	348.067822	4.491443	-0.005716	1.235566
29.534735	356.547575	4.496448	-0.005879	1.245415
30.285595	365.071079	4.501453	-0.006024	1.255220
30.449089	373.652626	4.506458	-0.006061	1.264901
30.851626	382.203356	4.511462	-0.006142	1.274520
31.442179	390.681716	4.516467	-0.006257	1.284021
31.877856	399.182136	4.521472	-0.006344	1.293449
32.505369	407.645265	4.526477	-0.006467	1.302802
32.939385	416.210405	4.531482	-0.006553	1.312163
33.429699	424.685403	4.536486	-0.006650	1.321371
33.802112	433.122713	4.541491	-0.006726	1.330454
34.171675	441.535586	4.546496	-0.006800	1.339449
34.786608	449.910442	4.551501	-0.006920	1.348387
35.160355	458.320200	4.556506	-0.006996	1.357260
35.958441	466.623023	4.561510	-0.007150	1.366038
36.867118	474.959890	4.566515	-0.007325	1.374814
37.142219	483.353610	4.571520	-0.007382	1.383483
37.669396	491.748383	4.576525	-0.007486	1.392143
38.282147	500.064669	4.581530	-0.007605	1.400683
38.815573	508.408886	4.586534	-0.007710	1.409187
39.082380	516.798330	4.591539	-0.007766	1.417640
39.517278	525.112515	4.596544	-0.007852	1.425996
40.134451	533.439460	4.601549	-0.007973	1.434345
40.514975	541.759019	4.606554	-0.008049	1.442600
40.682217	550.114317	4.611558	-0.008086	1.450809
41.265653	558.402215	4.616563	-0.008201	1.458972
41.733033	566.693086	4.621568	-0.008293	1.467075
42.172088	575.046200	4.626573	-0.008381	1.475188
42.832162	583.275411	4.631578	-0.008509	1.483172
43.479039	591.521666	4.636582	-0.008635	1.491128
43.915075	599.817589	4.641587	-0.008722	1.499055
44.098599	608.113915	4.646592	-0.008762	1.506903
44.498339	616.405540	4.651597	-0.008842	1.514738
44.832578	624.662916	4.656602	-0.008910	1.522491
45.332930	632.905847	4.661606	-0.009009	1.530216
45.846244	641.162408	4.666611	-0.009110	1.537916
46.191338	649.403338	4.671616	-0.009180	1.545539
46.765929	657.659394	4.676621	-0.009292	1.553172
47.044864	665.900762	4.681626	-0.009350	1.560710
47.447861	674.131739	4.686630	-0.009431	1.568221
47.771105	682.386936	4.691635	-0.009496	1.575706
48.128960	690.595117	4.696640	-0.009569	1.583119
48.948366	698.770224	4.701645	-0.009727	1.590533
49.371312	706.996102	4.706650	-0.009811	1.597902
49.730031	715.209239	4.711654	-0.009883	1.605216
49.802839	723.500828	4.716659	-0.009903	1.612525
50.484725	731.650133	4.721664	-0.010035	1.619763
51.066196	739.846495	4.726669	-0.010149	1.626994
51.259507	748.146016	4.731674	-0.010191	1.634230
51.793148	756.306336	4.736678	-0.010296	1.641360
52.595957	764.438616	4.741683	-0.010451	1.648471
52.843659	772.663373	4.746688	-0.010502	1.655556
53.155085	780.874330	4.751693	-0.010566	1.662607
53.395568	789.080999	4.756698	-0.010616	1.669615
53.678090	797.282523	4.761702	-0.010674	1.676595
54.078439	805.450732	4.766707	-0.010755	1.683533
54.479133	813.617463	4.771712	-0.010835	1.690442
55.264350	821.762745	4.776717	-0.010987	1.697355
55.725157	829.929228	4.781722	-0.011078	1.704215
56.345706	838.102079	4.786726	-0.011199	1.711074
56.526146	846.343023	4.791731	-0.011238	1.717903
56.633765	854.517784	4.796736	-0.011264	1.724642
57.010664	862.703200	4.801741	-0.011340	1.731398
57.464752	870.852766	4.806746	-0.011430	1.738109
57.930945	879.001844	4.811750	-0.011522	1.744794
58.150179	887.210883	4.816755	-0.011568	1.751471
58.727545	895.335480	4.821760	-0.011682	1.758100
59.137334	903.487920	4.826765	-0.011763	1.764705
59.372088	911.673426	4.831770	-0.011813	1.771290
59.813581	919.807899	4.836774	-0.011900	1.777835
60.232388	927.947620	4.841779	-0.011984	1.784357
60.451338	936.146218	4.846784	-0.012030	1.790878
60.786324	944.334169	4.851789	-0.012098	1.797381
61.138852	952.456138	4.856794	-0.012169	1.803810
61.424423	960.584079	4.861798	-0.012228	1.810213
61.861077	968.742408	4.866803	-0.012315	1.816635
62.230033	976.841602	4.871808	-0.012389	1.822981
62.602129	984.997754	4.876813	-0.012464	1.829349
63.113237	993.121246	4.881818	-0.012565	1.835685
63.609011	1001.224693	4.886822	-0.012663	1.841983
63.829198	1009.402723	4.891827	-0.012709	1.848284
64.203146	1017.548321	4.896832	-0.012784	1.854557
64.567786	1025.679180	4.901837	-0.012858	1.860796
64.921204	1033.805027	4.906842	-0.012929	1.867009
65.204692	1041.983425	4.911846	-0.012987	1.873232
65.609574	1050.102622	4.916851	-0.013068	1.879405
65.765906	1058.223539	4.921856	-0.013103	1.885530
66.313110	1066.343095	4.926861	-0.013210	1.891679
66.284415	1074.522418	4.931866	-0.013211	1.897787
66.666273	1082.608728	4.936870	-0.013287	1.903852
66.983843	1090.748195	4.941875	-0.013352	1.909930
67.234580	1098.876892	4.946880	-0.013404	1.915974
67.576883	1106.987994	4.951885	-0.013474	1.921995
67.856788	1115.108546	4.956890	-0.013531	1.927998
68.465671	1123.195724	4.961894	-0.013650	1.933994
68.895293	1131.314344	4.966899	-0.013736	1.939974
69.200543	1139.423882	4.971904	-0.013798	1.945916
69.610541	1147.593573	4.976909	-0.013880	1.951894
69.778706	1155.741376	4.981914	-0.013917	1.957812
69.790420	1163.850146	4.986918	-0.013924	1.963667
70.448983	1171.916429	4.991923	-0.014053	1.969544
70.783747	1180.023917	4.996928	-0.014120	1.975398
71.365035	1188.103926	5.001933	-0.014234	1.981241
71.569348	1196.215997	5.006938	-0.014278	1.987050
72.331515	1204.279375	5.011942	-0.014425	1.992866
72.382989	1212.439440	5.016947	-0.014440	1.998658
72.641769	1220.538336	5.021952	-0.014494	2.004413
73.182652	1228.629601	5.026957	-0.014600	2.010174
73.529570	1236.737662	5.031962	-0.014670	2.015911
73.719889	1244.864163	5.036966	-0.014711	2.021628
74.125474	1252.971356	5.041971	-0.014792	2.027338
74.358796	1261.107400	5.046976	-0.014841	2.033034
74.724918	1269.196565	5.051981	-0.014915	2.038695
74.948798	1277.290869	5.056986	-0.014962	2.044329
75.035409	1285.412245	5.061990	-0.014984	2.049953
75.381008	1293.520780	5.066995	-0.015054	2.055578
75.678506	1301.588840	5.072000	-0.015115	2.061155
76.156252	1309.676145	5.077005	-0.015209	2.066749
76.433935	1317.797126	5.082010	-0.015266	2.072330
76.604469	1325.898786	5.087014	-0.015304	2.077872
77.024835	1333.970929	5.092019	-0.015387	2.083405
77.147570	1342.078183	5.097024	-0.015416	2.088916
77.648013	1350.174315	5.102029	-0.015515	2.094443
77.893696	1358.259449	5.107034	-0.015566	2.099923
77.994556	1366.360866	5.112038	-0.015590	2.105386
78.265409	1374.511232	5.117043	-0.015646	2.110883
78.573425	1382.611176	5.122048	-0.015709	2.116336
78.734240	1390.690294	5.127053	-0.015744	2.121747
78.998753	1398.756473	5.132058	-0.015799	2.127146
79.332695	1406.836908	5.137062	-0.015867	2.132546
79.613476	1414.925920	5.142067	-0.015925	2.137934
79.806073	1422.996669	5.147072	-0.015966	2.143288
80.038576	1431.099110	5.152077	-0.016015	2.148652
80.467236	1439.189191	5.157082	-0.016100	2.154014
80.669234	1447.266629	5.162086	-0.016143	2.159333
81.156523	1455.303406	5.167091	-0.016239	2.164639
81.434048	1463.404036	5.172096	-0.016297	2.169953
81.955830	1471.488813	5.177101	-0.016399	2.175267
82.252170	1479.565640	5.182106	-0.016460	2.180542
82.568566	1487.638437	5.187110	-0.016524	2.185804
83.029597	1495.750333	5.192115	-0.016616	2.191091
83.385360	1503.848120	5.197120	-0.016688	2.196346
83.539557	1511.926039	5.202125	-0.016722	2.201558
84.111582	1519.957968	5.207130	-0.016834	2.206766
84.148498	1528.074662	5.212134	-0.016846	2.211967
84.613445	1536.147367	5.217139	-0.016938	2.217167
84.709761	1544.229852	5.222144	-0.016962	2.222327
85.189854	1552.290406	5.227149	-0.017057	2.227496
85.407645	1560.400869	5.232154	-0.017103	2.232661
85.617140	1568.467498	5.237158	-0.017147	2.237786
85.993320	1576.532966	5.242163	-0.017223	2.242913
86.262961	1584.612436	5.247168	-0.017278	2.248027
86.492638	1592.715829	5.252173	-0.017327	2.253141
86.750082	1600.799565	5.257178	-0.017380	2.258234
87.072068	1608.849080	5.262182	-0.017446	2.263300
87.326235	1616.948551	5.267187	-0.017498	2.268379
87.728860	1625.068887	5.272192	-0.017579	2.273473
87.972687	1633.139689	5.277197	-0.017630	2.278511
88.108175	1641.190334	5.282202	-0.017661	2.283515
88.558305	1649.215107	5.287206	-0.017750	2.288520
89.083244	1657.290240	5.292211	-0.017853	2.293551
89.090071	1665.380923	5.297216	-0.017860	2.298537
89.336900	1673.443525	5.302221	-0.017911	2.303515
89.493224	1681.538709	5.307226	-0.017946	2.308494
89.908062	1689.597717	5.312230	-0.018029	2.313462
90.456773	1697.621505	5.317235	-0.018136	2.318410
90.357518	1705.718985	5.322240	-0.018123	2.323337
90.626139	1713.794494	5.327245	-0.018179	2.328271
90.988145	1721.862001	5.332250	-0.018252	2.333198
91.226151	1729.922910	5.337254	-0.018302	2.338100
91.321671	1738.026715	5.342259	-0.018325	2.343005
91.450829	1746.093536	5.347264	-0.018355	2.347881
91.765933	1754.183473	5.352269	-0.018419	2.352776
92.166484	1762.224817	5.357274	-0.018499	2.357638
92.323268	1770.269016	5.362278	-0.018533	2.362473
92.402136	1778.368262	5.367283	-0.018554	2.367324
92.553148	1786.433641	5.372288	-0.018587	2.372150
93.143903	1794.466172	5.377293	-0.018703	2.376983
93.447827	1802.513201	5.382298	-0.018765	2.381791
93.450548	1810.608899	5.387302	-0.018771	2.386594
93.593562	1818.710331	5.392307	-0.018803	2.391402
94.144800	1826.723128	5.397312	-0.018911	2.396181
94.501747	1834.778215	5.402317	-0.018983	2.400959
94.864007	1842.832957	5.407322	-0.019056	2.405728
95.374762	1850.868219	5.412326	-0.019157	2.410488
95.629387	1858.980916	5.417331	-0.019210	2.415263
95.774113	1867.040292	5.422336	-0.019242	2.419990
96.065332	1875.107638	5.427341	-0.019302	2.424723
96.423123	1883.166862	5.432346	-0.019374	2.429447
96.398760	1891.337876	5.437350	-0.019375	2.434198
96.747384	1899.362622	5.442355	-0.019445	2.438883
97.127631	1907.357069	5.447360	-0.019522	2.443544
97.267634	1915.427796	5.452365	-0.019553	2.448221
97.523503	1923.497500	5.457370	-0.019606	2.452898
97.704227	1931.541635	5.462374	-0.019645	2.457546
98.174388	1939.576837	5.467379	-0.019738	2.462201
98.259872	1947.649504	5.472384	-0.019760	2.466840
98.385919	1955.751782	5.477389	-0.019789	2.471491
98.802199	1963.784322	5.482394	-0.019872	2.476114
98.837431	1971.839275	5.487398	-0.019884	2.480713
99.144876	1979.894702	5.492403	-0.019947	2.485324
99.536690	1987.922474	5.497408	-0.020025	2.489917
99.717848	1996.014631	5.502413	-0.020064	2.494523
99.778236	2004.083141	5.507418	-0.020081	2.499097
100.018182	2012.121194	5.512422	-0.020131	2.503660
100.586355	2020.162769	5.517427	-0.020242	2.508239
100.701301	2028.272472	5.522432	-0.020269	2.512816
100.901337	2036.332201	5.527437	-0.020312	2.517362
101.302459	2044.356058	5.532442	-0.020392	2.521895
101.368517	2052.396824	5.537446	-0.020410	2.526405
101.486434	2060.501527	5.542451	-0.020438	2.530946
102.079472	2068.497491	5.547456	-0.020553	2.535452
102.305586	2076.561582	5.552461	-0.020601	2.539962
102.526096	2084.602389	5.557466	-0.020648	2.544450
102.840597	2092.649810	5.562470	-0.020712	2.548941
103.133230	2100.762040	5.567475	-0.020772	2.553458
103.173606	2108.808983	5.572480	-0.020785	2.557914
103.288040	2116.864578	5.577485	-0.020811	2.562371
103.537000	2124.905948	5.582490	-0.020863	2.566823
103.914209	2132.948663	5.587494	-0.020939	2.571276
104.274684	2141.019612	5.592499	-0.021012	2.575736
104.581373	2149.041761	5.597504	-0.021074	2.580157
104.788614	2157.101482	5.602509	-0.021118	2.584585
105.057548	2165.162280	5.607514	-0.021174	2.589010
105.161689	2173.392809	5.612518	-0.021199	2.593508
105.734639	2181.398132	5.617523	-0.021311	2.597908
105.942661	2189.384207	5.622528	-0.021355	2.602265
106.194887	2197.416854	5.627533	-0.021408	2.606643
106.656507	2205.440864	5.632538	-0.021499	2.611024
106.565445	2213.533136	5.637542	-0.021488	2.615396
106.921641	2221.553937	5.642547	-0.021559	2.619753
107.075229	2229.583271	5.647552	-0.021593	2.624093
107.590472	2237.619883	5.652557	-0.021695	2.628454
107.768499	2245.691437	5.657562	-0.021734	2.632804
107.947888	2253.725627	5.662566	-0.021772	2.637128
108.391084	2261.759322	5.667571	-0.021860	2.641461
108.423388	2269.803210	5.672576	-0.021872	2.645765
108.822638	2277.839795	5.677581	-0.021952	2.650082
109.250362	2285.903829	5.682586	-0.022037	2.654409
109.206488	2293.964380	5.687590	-0.022034	2.658696
109.487848	2302.015279	5.692595	-0.022092	2.662992
110.053355	2310.006441	5.697600	-0.022203	2.667268
110.431921	2318.091917	5.702605	-0.022279	2.671575
110.461972	2326.199328	5.707610	-0.022290	2.675864
110.589608	2334.225673	5.712614	-0.022319	2.680110
111.102888	2342.213389	5.717619	-0.022420	2.684353
111.204892	2350.264960	5.722624	-0.022445	2.688597
111.246177	2358.381248	5.727629	-0.022458	2.692864
111.716740	2366.380095	5.732634	-0.022551	2.697090
111.502124	2374.473008	5.737638	-0.022517	2.701315
111.916679	2382.478409	5.742643	-0.022599	2.705527
112.014863	2390.528490	5.747648	-0.022623	2.709737
112.715266	2398.545426	5.752653	-0.022759	2.713960
113.118770	2406.601747	5.757658	-0.022839	2.718178
113.133638	2414.634834	5.762662	-0.022848	2.722354
113.510978	2422.692486	5.767667	-0.022923	2.726559
113.819018	2430.729432	5.772672	-0.022986	2.730741
114.258485	2438.776568	5.777677	-0.023074	2.734931
114.206355	2446.875831	5.782682	-0.023069	2.739111
114.288261	2454.909784	5.787686	-0.023090	2.743259
114.554170	2462.966370	5.792691	-0.023145	2.747424
114.806969	2471.033850	5.797696	-0.023198	2.751587
115.198159	2479.112619	5.802701	-0.023276	2.755758
115.280309	2487.125600	5.807706	-0.023297	2.759871
115.402706	2495.129382	5.812710	-0.023325	2.763974
115.834213	2503.163935	5.817715	-0.023411	2.768106
116.293314	2511.181804	5.822720	-0.023502	2.772225
116.482974	2519.253144	5.827725	-0.023543	2.776349
116.738948	2527.288953	5.832730	-0.023596	2.780453
116.889225	2535.287587	5.837734	-0.023629	2.784525
117.378956	2543.363898	5.842739	-0.023726	2.788651
117.333317	2551.449796	5.847744	-0.023723	2.792744
117.577880	2559.475012	5.852749	-0.023774	2.796817
117.842067	2567.514753	5.857754	-0.023829	2.800893
117.955267	2575.511302	5.862758	-0.023855	2.804932
118.055679	2583.598477	5.867763	-0.023879	2.809010
118.336517	2591.637570	5.872768	-0.023937	2.813069
118.513464	2599.696013	5.877773	-0.023976	2.817125
118.635632	2607.761242	5.882778	-0.024004	2.821176
118.750725	2615.782162	5.887782	-0.024031	2.825199
119.090552	2623.827653	5.892787	-0.024100	2.829240
119.227878	2631.892297	5.897792	-0.024131	2.833274
119.675236	2639.911910	5.902797	-0.024219	2.837298
119.946087	2647.933726	5.907802	-0.024275	2.841306
120.003095	2655.959243	5.912806	-0.024291	2.845299
120.371691	2664.000425	5.917811	-0.024365	2.849311
120.646397	2672.039821	5.922816	-0.024422	2.853312
120.958099	2680.089638	5.927821	-0.024486	2.857314
121.108546	2688.129275	5.932826	-0.024519	2.861296
121.360877	2696.135829	5.937830	-0.024572	2.865263
121.766929	2704.182627	5.942835	-0.024653	2.869252
121.800590	2712.261658	5.947840	-0.024664	2.873230
122.118654	2720.286399	5.952845	-0.024729	2.877192
122.410617	2728.320845	5.957850	-0.024789	2.881152
122.546131	2736.338071	5.962854	-0.024820	2.885090
122.761389	2744.416169	5.967859	-0.024865	2.889056
123.032930	2752.454501	5.972864	-0.024921	2.893000
123.064126	2760.526784	5.977869	-0.024933	2.896943
123.427362	2768.553451	5.982874	-0.025006	2.900876
123.754035	2776.536220	5.987878	-0.025072	2.904780
123.906739	2784.634573	5.992883	-0.025106	2.908725
123.866749	2792.742077	5.997888	-0.025104	2.912660
124.204101	2800.787464	6.002893	-0.025172	2.916579
124.347936	2808.788972	6.007898	-0.025205	2.920461
124.529945	2816.759560	6.012902	-0.025244	2.924325
125.060120	2824.781633	6.017907	-0.025348	2.928227
125.203709	2832.827112	6.022912	-0.025380	2.932115
125.551123	2840.883193	6.027917	-0.025451	2.936013
125.764338	2848.893982	6.032922	-0.025496	2.939878
126.154877	2856.900726	6.037926	-0.025574	2.943744
126.445537	2864.962905	6.042931	-0.025633	2.947627
126.434333	2873.038548	6.047936	-0.025637	2.951496
126.779883	2881.073194	6.052941	-0.025707	2.955358
127.038552	2889.084106	6.057946	-0.025760	2.959199
127.246407	2897.095329	6.062950	-0.025805	2.963033
127.459692	2905.172180	6.067955	-0.025850	2.966893
127.527692	2913.208304	6.072960	-0.025868	2.970722
127.954283	2921.244057	6.077965	-0.025953	2.974564
127.902343	2929.337612	6.082970	-0.025949	2.978403
128.129800	2937.328775	6.087974	-0.025996	2.982204
128.461713	2945.382473	6.092979	-0.026064	2.986034
128.573380	2953.401397	6.097984	-0.026090	2.989832
128.853132	2961.470301	6.102989	-0.026148	2.993657
129.408346	2969.486741	6.107994	-0.026256	2.997466
129.509783	2977.501949	6.112998	-0.026281	3.001247
129.467976	2985.548411	6.118003	-0.026278	3.005031
129.692003	2993.565045	6.123008	-0.026326	3.008809
129.899018	3001.644258	6.128013	-0.026370	3.012611
130.053640	3009.699966	6.133018	-0.026404	3.016395
130.311671	3017.679643	6.138022	-0.026458	3.020143
130.742556	3025.701423	6.143027	-0.026543	3.023915
130.714362	3033.750563	6.148032	-0.026543	3.027672
130.825509	3041.836047	6.153037	-0.026570	3.031449
131.221676	3049.866514	6.158042	-0.026649	3.035208
131.395614	3057.867755	6.163046	-0.026687	3.038939
131.556041	3065.907889	6.168051	-0.026722	3.042683
131.525488	3073.957557	6.173056	-0.026722	3.046417
132.041742	3081.960021	6.178061	-0.026823	3.050151
132.157136	3090.029354	6.183066	-0.026850	3.053892
132.221225	3098.056491	6.188070	-0.026868	3.057607
132.574750	3106.080658	6.193075	-0.026939	3.061329
132.975251	3114.063240	6.198080	-0.027019	3.065030
133.148084	3122.121664	6.203085	-0.027057	3.068750
133.452792	3130.227439	6.208090	-0.027119	3.072494
133.654030	3138.272903	6.213094	-0.027162	3.076201
133.681629	3146.291373	6.218099	-0.027173	3.079883
133.991429	3154.266999	6.223104	-0.027236	3.083554
134.166534	3162.301401	6.228109	-0.027274	3.087241
134.354837	3170.359881	6.233114	-0.027314	3.090935
134.328910	3178.412774	6.238118	-0.027315	3.094612
134.871776	3186.405690	6.243123	-0.027422	3.098284
134.806498	3194.439961	6.248128	-0.027415	3.101943
134.946988	3202.480228	6.253133	-0.027447	3.105609
135.367067	3210.482870	6.258138	-0.027530	3.109266
135.825200	3218.526441	6.263142	-0.027621	3.112939
135.897807	3226.608523	6.268147	-0.027640	3.116608
135.982297	3234.615556	6.273152	-0.027661	3.120240
136.397504	3242.617783	6.278157	-0.027744	3.123879
136.584762	3250.668037	6.283162	-0.027784	3.127526
136.827717	3258.695987	6.288166	-0.027835	3.131161
137.232955	3266.736092	6.293171	-0.027916	3.134804
137.328346	3274.768413	6.298176	-0.027939	3.138426
137.517684	3282.785560	6.303181	-0.027980	3.142041
137.817671	3290.817875	6.308186	-0.028041	3.145664
137.896870	3298.861730	6.313190	-0.028062	3.149277
138.194959	3306.942267	6.318195	-0.028123	3.152913
138.461648	3314.978145	6.323200	-0.028178	3.156523
138.689075	3322.951753	6.328205	-0.028226	3.160099
138.817524	3331.000064	6.333210	-0.028255	3.163700
139.006231	3338.995775	6.338214	-0.028296	3.167277
139.085106	3347.068714	6.343219	-0.028316	3.170879
139.224771	3355.105021	6.348224	-0.028347	3.174463
139.528367	3363.124161	6.353229	-0.028409	3.178042
139.555253	3371.188945	6.358234	-0.028420	3.181626
139.951783	3379.156983	6.363238	-0.028499	3.185178
140.195614	3387.230495	6.368243	-0.028550	3.188767
140.250765	3395.269872	6.373248	-0.028566	3.192329
140.775424	3403.296101	6.378253	-0.028669	3.195900
141.049070	3411.313031	6.383258	-0.028725	3.199453
141.187107	3419.327822	6.388262	-0.028756	3.202995
141.408760	3427.390414	6.393267	-0.028803	3.206558
141.565298	3435.415034	6.398272	-0.028838	3.210097
141.762877	3443.473135	6.403277	-0.028880	3.213649
141.981168	3451.497062	6.408282	-0.028926	3.217183
142.201546	3459.496983	6.413286	-0.028973	3.220703
142.374208	3467.514521	6.418291	-0.029010	3.224224
142.635222	3475.532648	6.423296	-0.029064	3.227745
143.045351	3483.605023	6.428301	-0.029146	3.231292
143.348082	3491.702924	6.433306	-0.029208	3.234842
143.403798	3499.674654	6.438310	-0.029224	3.238323
143.714246	3507.685816	6.443315	-0.029287	3.241828
143.902888	3515.696284	6.448320	-0.029328	3.245324
143.970374	3523.729559	6.453325	-0.029346	3.248821
144.050861	3531.776082	6.458330	-0.029366	3.252320
144.318542	3539.820569	6.463334	-0.029422	3.255823
144.622267	3547.828757	6.468339	-0.029484	3.259307
144.632870	3555.860272	6.473344	-0.029491	3.262786
144.878904	3563.888228	6.478349	-0.029542	3.266269
145.087629	3571.920334	6.483354	-0.029587	3.269748
145.380466	3579.948381	6.488358	-0.029647	3.273225
145.725801	3587.984691	6.493363	-0.029717	3.276704
145.986399	3595.979392	6.498368	-0.029771	3.280159
146.059515	3604.009778	6.503373	-0.029790	3.283617
146.223350	3612.068096	6.508378	-0.029826	3.287088
146.300466	3620.093366	6.513382	-0.029845	3.290537
146.563931	3628.144574	6.518387	-0.029900	3.294001
146.716873	3636.164008	6.523392	-0.029934	3.297443
146.961741	3644.188054	6.528397	-0.029985	3.300887
147.216818	3652.191936	6.533402	-0.030038	3.304320
147.267915	3660.229761	6.538406	-0.030053	3.307755
147.505174	3668.301878	6.543411	-0.030103	3.311209
147.647053	3676.338247	6.548416	-0.030135	3.314640
147.801908	3684.338591	6.553421	-0.030169	3.318052
148.026195	3692.355806	6.558426	-0.030216	3.321471
148.405946	3700.323591	6.563430	-0.030292	3.324871
148.794590	3708.366635	6.568435	-0.030370	3.328300
148.990659	3716.414442	6.573440	-0.030412	3.331720
149.114498	3724.473995	6.578445	-0.030441	3.335139
149.426211	3732.501853	6.583450	-0.030504	3.338548
149.580630	3740.491936	6.588454	-0.030538	3.341932
149.892767	3748.544526	6.593459	-0.030602	3.345344
149.868780	3756.582095	6.598464	-0.030603	3.348734
150.096505	3764.627505	6.603469	-0.030651	3.352134
150.347153	3772.673283	6.608474	-0.030703	3.355530
150.408240	3780.667188	6.613478	-0.030720	3.358895
150.672082	3788.704488	6.618483	-0.030774	3.362282
150.960693	3796.704741	6.623488	-0.030834	3.365650
151.012408	3804.730454	6.628493	-0.030849	3.369018
151.516944	3812.791169	6.633498	-0.030948	3.372413
151.386414	3820.849435	6.638502	-0.030929	3.375780
151.765018	3828.849246	6.643507	-0.031005	3.379138
152.017828	3836.861142	6.648512	-0.031058	3.382494
152.168452	3844.909981	6.653517	-0.031091	3.385857
152.221394	3852.944426	6.658522	-0.031107	3.389208
152.451359	3861.019951	6.663526	-0.031155	3.392579
152.895116	3869.065383	6.668531	-0.031243	3.395941
152.790390	3877.037973	6.673536	-0.031229	3.399251
152.902507	3885.025731	6.678541	-0.031255	3.402571
153.433944	3893.035305	6.683546	-0.031360	3.405912
153.438480	3901.037321	6.688550	-0.031366	3.409228
153.781890	3909.107271	6.693555	-0.031436	3.412580
153.850258	3917.150717	6.698560	-0.031454	3.415909
154.029600	3925.153558	6.703565	-0.031493	3.419221
154.117408	3933.181640	6.708570	-0.031514	3.422538
154.237354	3941.215670	6.713574	-0.031542	3.425854
154.605811	3949.243973	6.718579	-0.031616	3.429174
154.544653	3957.298724	6.723584	-0.031610	3.432487
155.054732	3965.321399	6.728589	-0.031711	3.435802
155.252050	3973.300756	6.733594	-0.031753	3.439086
155.261646	3981.354106	6.738598	-0.031760	3.442391
155.413577	3989.377754	6.743603	-0.031794	3.445686
155.746322	3997.380799	6.748608	-0.031862	3.448974
155.853723	4005.451062	6.753613	-0.031887	3.452280
156.108836	4013.501174	6.758618	-0.031940	3.455579
156.117336	4021.463425	6.763622	-0.031947	3.458831
156.429455	4029.517559	6.768627	-0.032011	3.462127
156.612524	4037.507077	6.773632	-0.032050	3.465390
156.574321	4045.579395	6.778637	-0.032049	3.468675
156.980827	4053.612456	6.783642	-0.032130	3.471957
157.164981	4061.662508	6.788646	-0.032170	3.475234
157.373911	4069.651368	6.793651	-0.032214	3.478485
157.352926	4077.684444	6.798656	-0.032215	3.481743
157.647197	4085.643173	6.803661	-0.032276	3.484978
157.779977	4093.719329	6.808666	-0.032306	3.488253
157.831049	4101.737740	6.813670	-0.032321	3.491498
158.301998	4109.768677	6.818675	-0.032414	3.494759
158.351020	4117.807763	6.823680	-0.032429	3.498006
158.461681	4125.822454	6.828685	-0.032455	3.501243
158.828084	4133.801518	6.833690	-0.032528	3.504470
159.036234	4141.840704	6.838694	-0.032573	3.507713
159.222781	4149.892210	6.843699	-0.032613	3.510958
159.393263	4157.911304	6.848704	-0.032650	3.514186
159.792792	4165.928037	6.853709	-0.032730	3.517417
159.922436	4173.949660	6.858714	-0.032760	3.520639
159.861510	4181.945728	6.863718	-0.032754	3.523842
160.099564	4190.022977	6.868723	-0.032804	3.527084
160.398456	4198.012577	6.873728	-0.032865	3.530289
160.486411	4206.058409	6.878733	-0.032886	3.533508
160.742133	4214.117702	6.883738	-0.032940	3.536734
161.035150	4222.101806	6.888742	-0.033000	3.539928
161.066177	4230.162355	6.893747	-0.033011	3.543141
161.259992	4238.184294	6.898752	-0.033052	3.546342
161.475312	4246.226096	6.903757	-0.033098	3.549548
161.791780	4254.325081	6.908762	-0.033162	3.552777
161.589588	4262.360119	6.913766	-0.033130	3.555962
161.939485	4270.309298	6.918771	-0.033201	3.559126
162.113615	4278.307897	6.923776	-0.033239	3.562302
162.276096	4286.311428	6.928781	-0.033274	3.565477
162.577587	4294.344286	6.933786	-0.033336	3.568664
162.778807	4302.368934	6.938790	-0.033379	3.571843
163.016007	4310.413214	6.943795	-0.033429	3.575027
163.080205	4318.416496	6.948800	-0.033446	3.578188
163.608900	4326.415978	6.953805	-0.033550	3.581357
163.677499	4334.468160	6.958810	-0.033568	3.584531
163.616719	4342.490086	6.963814	-0.033562	3.587687
164.077670	4350.525780	6.968819	-0.033654	3.590860
164.088579	4358.551989	6.973824	-0.033661	3.594014
164.065498	4366.581342	6.978829	-0.033662	3.597166
164.304765	4374.585365	6.983834	-0.033712	3.600312
164.696596	4382.540948	6.988838	-0.033791	3.603440
164.742062	4390.619299	6.993843	-0.033805	3.606604
164.690482	4398.628643	6.998848	-0.033801	3.609736
164.996540	4406.677872	7.003853	-0.033863	3.612890
165.376261	4414.740265	7.008858	-0.033939	3.616049
165.395340	4422.670438	7.013862	-0.033948	3.619144
165.656845	4430.746585	7.018867	-0.034002	3.622299
165.822205	4438.762070	7.023872	-0.034039	3.625426
166.134665	4446.786295	7.028877	-0.034102	3.628557
166.282535	4454.877294	7.033882	-0.034135	3.631706
166.307711	4462.918003	7.038886	-0.034146	3.634831
166.555395	4470.923643	7.043891	-0.034197	3.637945
166.656085	4478.912610	7.048896	-0.034221	3.641045
167.076450	4486.882336	7.053901	-0.034305	3.644145
167.223171	4494.960986	7.058906	-0.034338	3.647276
167.266824	4502.981053	7.063910	-0.034351	3.650379
167.361190	4511.044102	7.068915	-0.034375	3.653498
167.582708	4519.077907	7.073920	-0.034421	3.656606
167.632018	4527.042134	7.078925	-0.034436	3.659680
167.765192	4535.091660	7.083930	-0.034466	3.662786
167.995572	4543.070954	7.088934	-0.034515	3.665865
168.331351	4551.109202	7.093939	-0.034583	3.668967
168.477624	4559.159042	7.098944	-0.034615	3.672066
168.617190	4567.167424	7.103949	-0.034647	3.675146
168.967975	4575.177412	7.108954	-0.034717	3.678230
169.062859	4583.204843	7.113958	-0.034741	3.681311
169.247308	4591.211899	7.118963	-0.034780	3.684384
169.416584	4599.253656	7.123968	-0.034817	3.687467
169.494772	4607.279676	7.128973	-0.034837	3.690540
169.763424	4615.330918	7.133978	-0.034893	3.693624
169.919944	4623.323603	7.138982	-0.034928	3.696680
170.111637	4631.349321	7.143987	-0.034969	3.699748
170.024890	4639.364765	7.148992	-0.034958	3.702802
170.239759	4647.374522	7.153997	-0.035004	3.705858
170.601691	4655.433134	7.159002	-0.035076	3.708935
170.551617	4663.480124	7.164006	-0.035073	3.711994
170.517221	4671.557382	7.169011	-0.035072	3.715063
170.985337	4679.499557	7.174016	-0.035164	3.718090
171.242388	4687.504774	7.179021	-0.035218	3.721133
171.304021	4695.488798	7.184026	-0.035234	3.724161
171.384835	4703.520186	7.189030	-0.035255	3.727205
171.810959	4711.509811	7.194035	-0.035340	3.730239
172.033035	4719.563676	7.199040	-0.035387	3.733290
172.156423	4727.609808	7.204045	-0.035415	3.736333
172.497606	4735.619881	7.209050	-0.035484	3.739365
172.475856	4743.661897	7.214054	-0.035486	3.742398
172.768199	4751.677505	7.219059	-0.035545	3.745426
173.018275	4759.695741	7.224064	-0.035597	3.748452
172.930094	4767.750755	7.229069	-0.035587	3.751481
173.296492	4775.760785	7.234074	-0.035660	3.754501
173.345028	4783.755525	7.239078	-0.035675	3.757505
173.555786	4791.813254	7.244083	-0.035719	3.760535
173.763834	4799.814461	7.249088	-0.035764	3.763541
173.879563	4807.829487	7.254093	-0.035791	3.766547
174.081356	4815.862400	7.259098	-0.035834	3.769560
174.376392	4823.879465	7.264102	-0.035894	3.772567
174.467578	4831.937987	7.269107	-0.035917	3.775581
174.644610	4839.938446	7.274112	-0.035955	3.778574
174.835492	4847.978804	7.279117	-0.035996	3.781580
174.939626	4855.990667	7.284122	-0.036021	3.784570
174.943761	4864.017426	7.289126	-0.036027	3.787562
175.293152	4872.029086	7.294131	-0.036098	3.790553
175.379912	4880.105674	7.299136	-0.036119	3.793560
175.416096	4888.100150	7.304141	-0.036132	3.796533
175.778500	4896.102647	7.309146	-0.036204	3.799514
175.871545	4904.090445	7.314150	-0.036227	3.802481
175.963643	4912.131741	7.319155	-0.036250	3.805466
176.212987	4920.104461	7.324160	-0.036302	3.808426
176.363461	4928.188787	7.329165	-0.036335	3.811423
176.576752	4936.188960	7.334170	-0.036380	3.814388
176.720954	4944.212978	7.339174	-0.036413	3.817358
177.083228	4952.185070	7.344179	-0.036486	3.820311
177.120817	4960.249867	7.349184	-0.036498	3.823289
177.172752	4968.257499	7.354189	-0.036513	3.826244
177.441897	4976.295368	7.359194	-0.036569	3.829213
177.680596	4984.300629	7.364198	-0.036619	3.832166
177.630573	4992.377795	7.369203	-0.036615	3.835138
177.939295	5000.350881	7.374208	-0.036678	3.838076
178.402178	5008.365723	7.379213	-0.036770	3.841031
178.522217	5016.361980	7.384218	-0.036797	3.843969
178.356643	5024.380413	7.389222	-0.036772	3.846908
178.610000	5032.437757	7.394227	-0.036825	3.849867
178.975403	5040.459377	7.399232	-0.036898	3.852813
179.098101	5048.504167	7.404237	-0.036926	3.855760
179.274408	5056.509517	7.409242	-0.036965	3.858691
179.566001	5064.514693	7.414246	-0.037025	3.861623
179.829290	5072.537901	7.419251	-0.037079	3.864558
180.205679	5080.538041	7.424256	-0.037155	3.867485
180.196913	5088.586796	7.429261	-0.037158	3.870420
180.644219	5096.845793	7.434266	-0.037247	3.873438
180.709154	5104.836997	7.439270	-0.037265	3.876348
181.020550	5112.719665	7.444275	-0.037328	3.879222
181.091668	5120.740634	7.449280	-0.037347	3.882139
181.067719	5128.707415	7.454285	-0.037348	3.885033
181.295944	5136.744996	7.459290	-0.037396	3.887955
181.531794	5144.766796	7.464294	-0.037445	3.890869
181.805539	5152.800471	7.469299	-0.037502	3.893786
181.844331	5160.820768	7.474304	-0.037514	3.896691
182.036918	5168.774273	7.479309	-0.037556	3.899573
182.358347	5176.855700	7.484314	-0.037621	3.902502
182.344021	5184.842427	7.489318	-0.037624	3.905387
182.450871	5192.875480	7.494323	-0.037649	3.908290
182.519146	5200.941656	7.499328	-0.037667	3.911201
182.606688	5208.929726	7.504333	-0.037689	3.914083
182.831928	5216.959136	7.509338	-0.037737	3.916980
183.024028	5224.883508	7.514342	-0.037778	3.919836
183.354034	5232.976889	7.519347	-0.037845	3.922754
183.471772	5240.968186	7.524352	-0.037872	3.925628
183.673339	5248.953334	7.529357	-0.037915	3.928500
184.114210	5257.052445	7.534362	-0.038003	3.931415
184.175812	5265.022663	7.539366	-0.038020	3.934275
184.345320	5273.088306	7.544371	-0.038057	3.937169
184.576513	5281.067070	7.549376	-0.038105	3.940030
184.696231	5289.050286	7.554381	-0.038133	3.942890
184.851549	5297.094364	7.559386	-0.038167	3.945769
184.907325	5305.138801	7.564390	-0.038183	3.948645
185.036659	5313.192526	7.569395	-0.038213	3.951523
185.000228	5321.237520	7.574400	-0.038211	3.954393
185.329019	5329.236437	7.579405	-0.038278	3.957251
185.601008	5337.217738	7.584410	-0.038334	3.960099
185.662820	5345.214167	7.589414	-0.038351	3.962948
185.853063	5353.231280	7.594419	-0.038392	3.965803
186.138075	5361.256756	7.599424	-0.038451	3.968661
186.295455	5369.291588	7.604429	-0.038485	3.971519
186.491594	5377.338360	7.609434	-0.038527	3.974379
186.793737	5385.323506	7.614438	-0.038589	3.977217
186.843822	5393.339566	7.619443	-0.038604	3.980059
187.003901	5401.381798	7.624448	-0.038639	3.982911
187.146289	5409.381288	7.629453	-0.038671	3.985745
187.251044	5417.425370	7.634458	-0.038696	3.988592
187.323315	5425.453784	7.639462	-0.038715	3.991431
187.481822	5433.514924	7.644467	-0.038750	3.994282
187.773785	5441.519147	7.649472	-0.038810	3.997112
187.978889	5449.496840	7.654477	-0.038854	3.999929
188.220868	5457.534395	7.659482	-0.038904	4.002766
188.403582	5465.531679	7.664486	-0.038944	4.005586
188.539430	5473.569628	7.669491	-0.038974	4.008417
188.814127	5481.607977	7.674496	-0.039031	4.011249
189.123523	5489.635472	7.679501	-0.039094	4.014075
189.313384	5497.682978	7.684506	-0.039135	4.016904
189.288151	5505.627432	7.689510	-0.039136	4.019692
189.473676	5513.671389	7.694515	-0.039176	4.022517
189.502801	5521.706571	7.699520	-0.039187	4.025333
189.748736	5529.706708	7.704525	-0.039238	4.028139
190.064777	5537.766590	7.709530	-0.039302	4.030965
190.069902	5545.869858	7.714534	-0.039309	4.033799
190.326315	5553.858972	7.719539	-0.039362	4.036595
190.453812	5561.812779	7.724544	-0.039391	4.039375
190.559922	5569.802570	7.729549	-0.039416	4.042165
190.777563	5577.810199	7.734554	-0.039462	4.044961
190.955225	5585.825161	7.739558	-0.039501	4.047757
191.189355	5593.859507	7.744563	-0.039550	4.050559
191.275164	5601.886007	7.749568	-0.039571	4.053354
191.255265	5609.927000	7.754573	-0.039573	4.056150
191.581386	5617.921405	7.759578	-0.039639	4.058933
191.776334	5625.911587	7.764582	-0.039681	4.061711
192.141448	5633.895816	7.769587	-0.039754	4.064488
192.148118	5641.980506	7.774592	-0.039761	4.067292
192.280859	5649.962918	7.779597	-0.039791	4.070060
192.495520	5658.013324	7.784602	-0.039837	4.072852
192.700625	5666.028230	7.789606	-0.039880	4.075629
192.616327	5674.021515	7.794611	-0.039870	4.078392
193.025864	5682.038368	7.799616	-0.039952	4.081169
193.094951	5690.037355	7.804621	-0.039970	4.083933
193.294265	5698.123492	7.809626	-0.040013	4.086727
193.335851	5706.086574	7.814630	-0.040026	4.089474
193.633831	5714.134663	7.819635	-0.040087	4.092252
193.654670	5722.171982	7.824640	-0.040096	4.095021
193.784157	5730.163357	7.829645	-0.040126	4.097774
194.079875	5738.169171	7.834650	-0.040186	4.100532
194.182730	5746.179751	7.839654	-0.040211	4.103287
194.386703	5754.207348	7.844659	-0.040255	4.106048
194.499539	5762.266656	7.849664	-0.040281	4.108816
194.748179	5770.283520	7.854669	-0.040333	4.111570
194.920811	5778.339708	7.859674	-0.040370	4.114334
195.003325	5786.402040	7.864678	-0.040391	4.117097
195.406158	5794.335646	7.869683	-0.040472	4.119819
195.540695	5802.343963	7.874688	-0.040502	4.122560
195.358914	5810.355655	7.879693	-0.040474	4.125297
195.910514	5818.394101	7.884698	-0.040582	4.128051
195.893493	5826.394905	7.889702	-0.040584	4.130783
195.930993	5834.447532	7.894707	-0.040597	4.133531
196.187757	5842.512269	7.899712	-0.040650	4.136284
196.264326	5850.446923	7.904717	-0.040670	4.138989
196.536487	5858.513701	7.909722	-0.040726	4.141740
196.648295	5866.485216	7.914726	-0.040752	4.144454
196.932960	5874.531195	7.919731	-0.040811	4.147194
197.093497	5882.554826	7.924736	-0.040846	4.149923
197.140870	5890.578576	7.929741	-0.040860	4.152649
197.383942	5898.633021	7.934746	-0.040911	4.155385
197.522330	5906.577734	7.939750	-0.040942	4.158082
197.716714	5914.624323	7.944755	-0.040984	4.160812
197.774511	5922.633938	7.949760	-0.041000	4.163526
198.015340	5930.655501	7.954765	-0.041051	4.166244
198.244275	5938.692044	7.959770	-0.041099	4.168965
198.111120	5946.729486	7.964774	-0.041079	4.171681
198.458012	5954.747755	7.969779	-0.041149	4.174394
198.516338	5962.778205	7.974784	-0.041166	4.177106
198.762505	5970.741985	7.979789	-0.041217	4.179796
198.799093	5978.770679	7.984794	-0.041229	4.182504
199.042201	5986.784881	7.989798	-0.041280	4.185207
199.073581	5994.812171	7.994803	-0.041291	4.187911
199.071670	6002.837391	7.999808	-0.041296	4.190612
199.436973	6010.924736	8.004813	-0.041370	4.193336
199.763232	6018.976930	8.009818	-0.041436	4.196046
199.739533	6026.887493	8.014822	-0.041437	4.198702
200.153627	6034.912091	8.019827	-0.041520	4.201401
200.389461	6042.856366	8.024832	-0.041569	4.204068
200.229348	6050.886106	8.029837	-0.041545	4.206758
200.400847	6058.940511	8.034842	-0.041582	4.209458
200.731263	6066.980364	8.039846	-0.041649	4.212154
201.006516	6074.994525	8.044851	-0.041706	4.214838
201.175126	6082.983524	8.049856	-0.041743	4.217511
201.221021	6090.972952	8.054861	-0.041757	4.220181
201.488094	6099.003867	8.059866	-0.041812	4.222866
201.472113	6107.029708	8.064870	-0.041814	4.225544
201.724831	6115.060199	8.069875	-0.041867	4.228225
201.858431	6123.081590	8.074880	-0.041897	4.230900
201.691851	6131.117805	8.079885	-0.041872	4.233575
202.094470	6139.172587	8.084890	-0.041952	4.236260
202.304383	6147.097381	8.089894	-0.041997	4.238899
202.432216	6155.134754	8.094899	-0.042026	4.241572
202.650088	6163.113609	8.099904	-0.042072	4.244225
202.588059	6171.166572	8.104909	-0.042066	4.246899
203.027981	6179.155023	8.109914	-0.042153	4.249554
202.876555	6187.240423	8.114918	-0.042131	4.252234
203.198847	6195.265975	8.119923	-0.042196	4.254896
203.292847	6203.276545	8.124928	-0.042219	4.257550
203.312279	6211.244181	8.129933	-0.042228	4.260188
203.566620	6219.319943	8.134938	-0.042281	4.262861
203.697305	6227.305953	8.139942	-0.042311	4.265503
203.902191	6235.349826	8.144947	-0.042354	4.268162
204.009609	6243.373951	8.149952	-0.042380	4.270812
204.102269	6251.408231	8.154957	-0.042403	4.273464
204.286208	6259.493472	8.159962	-0.042442	4.276132
204.308934	6267.410799	8.164966	-0.042452	4.278741
204.487243	6275.465532	8.169971	-0.042491	4.281396
204.716259	6283.441506	8.174976	-0.042539	4.284023
204.673544	6291.492948	8.179981	-0.042536	4.286671
204.970634	6299.473395	8.184986	-0.042597	4.289297
205.232853	6307.513912	8.189990	-0.042651	4.291940
205.202011	6315.563875	8.194995	-0.042651	4.294583
205.147009	6323.555616	8.200000	-0.042646	4.297205
205.322956	6331.551378	8.205005	-0.042685	4.299829
205.697704	6339.574950	8.210010	-0.042760	4.302461
205.649614	6347.567927	8.215014	-0.042756	4.305078
205.791868	6355.624218	8.220019	-0.042788	4.307717
206.080807	6363.642923	8.225024	-0.042848	4.310342
206.247196	6371.667588	8.230029	-0.042884	4.312967
206.328763	6379.712558	8.235034	-0.042905	4.315596
206.420039	6387.670434	8.240038	-0.042927	4.318195
206.734699	6395.720905	8.245043	-0.042991	4.320824
206.882202	6403.692079	8.250048	-0.043024	4.323425
207.018054	6411.699042	8.255053	-0.043055	4.326035
207.230604	6419.731259	8.260058	-0.043100	4.328653
207.201697	6427.737274	8.265062	-0.043100	4.331259
207.634314	6435.821586	8.270067	-0.043186	4.333892
207.507180	6443.845257	8.275072	-0.043168	4.336500
207.784366	6451.756473	8.280077	-0.043225	4.339072
207.778590	6459.867946	8.285082	-0.043229	4.341706
207.744902	6467.803065	8.290086	-0.043228	4.344281
208.157880	6475.847222	8.295091	-0.043311	4.346893
208.214115	6483.861343	8.300096	-0.043327	4.349491
208.411425	6491.914043	8.305101	-0.043369	4.352101
208.554466	6500.007486	8.310106	-0.043401	4.354723
208.785184	6507.961272	8.315110	-0.043450	4.357298
208.900478	6515.943394	8.320115	-0.043476	4.359880
208.907936	6523.956575	8.325120	-0.043483	4.362469
209.146779	6531.916856	8.330125	-0.043533	4.365042
209.306576	6539.998587	8.335130	-0.043569	4.367652
209.379478	6547.981357	8.340134	-0.043588	4.370227
209.710198	6556.031824	8.345139	-0.043655	4.372825
209.931232	6564.042740	8.350144	-0.043701	4.375407
210.070832	6572.071625	8.355149	-0.043733	4.377993
210.321691	6580.086795	8.360154	-0.043785	4.380574
210.485075	6588.056919	8.365158	-0.043821	4.383139
210.186387	6596.082781	8.370163	-0.043771	4.385717
210.634286	6604.127288	8.375168	-0.043859	4.388304
210.631074	6612.104848	8.380173	-0.043864	4.390865
210.797475	6620.200934	8.385178	-0.043901	4.393464
210.784243	6628.182253	8.390182	-0.043904	4.396023
211.002695	6636.197445	8.395187	-0.043950	4.398593
211.350179	6644.225991	8.400192	-0.044020	4.401167
211.323521	6652.188485	8.405197	-0.044021	4.403716
211.589789	6660.247451	8.410202	-0.044076	4.406295
211.877241	6668.249381	8.415206	-0.044135	4.408855
211.786058	6676.278722	8.420211	-0.044123	4.411421
212.017297	6684.323287	8.425216	-0.044172	4.413991
212.385464	6692.333338	8.430221	-0.044246	4.416550
212.434383	6700.334479	8.435226	-0.044260	4.419102
212.313440	6708.385944	8.440230	-0.044243	4.421668
212.652769	6716.379306	8.445235	-0.044312	4.424217
212.942353	6724.385998	8.450240	-0.044371	4.426768
212.996882	6732.386131	8.455245	-0.044387	4.429314
213.317925	6740.499004	8.460250	-0.044452	4.431896
213.305233	6748.505543	8.465254	-0.044455	4.434441
213.437074	6756.483211	8.470259	-0.044485	4.436976
213.611259	6764.488524	8.475264	-0.044523	4.439519
213.695923	6772.486925	8.480269	-0.044544	4.442057
213.894698	6780.472661	8.485274	-0.044587	4.444591
213.946204	6788.513259	8.490278	-0.044602	4.447140
214.016946	6796.506986	8.495283	-0.044621	4.449672
214.295276	6804.562817	8.500288	-0.044678	4.452224
214.304071	6812.545854	8.505293	-0.044685	4.454750
214.750961	6820.646502	8.510298	-0.044774	4.457313
214.779195	6828.606921	8.515302	-0.044784	4.459829
214.766603	6836.637595	8.520307	-0.044787	4.462366
214.926879	6844.627273	8.525312	-0.044823	4.464889
215.165979	6852.656257	8.530317	-0.044873	4.467423
215.405559	6860.668109	8.535322	-0.044923	4.469950
215.351006	6868.748350	8.540326	-0.044918	4.472496
215.543360	6876.727342	8.545331	-0.044959	4.475010
215.939065	6884.736476	8.550336	-0.045039	4.477533
215.865780	6892.704664	8.555341	-0.045030	4.480040
215.914834	6900.749509	8.560346	-0.045045	4.482569
216.069409	6908.736231	8.565351	-0.045079	4.485080
216.205328	6916.776405	8.570355	-0.045110	4.487605
216.600852	6924.784783	8.575360	-0.045189	4.490121
216.595168	6932.832556	8.580365	-0.045194	4.492645
216.886609	6940.870093	8.585370	-0.045253	4.495166
216.949306	6948.864562	8.590375	-0.045270	4.497672
217.193912	6956.854888	8.595379	-0.045321	4.500175
217.397897	6964.908991	8.600384	-0.045365	4.502697
217.376697	6972.853864	8.605389	-0.045366	4.505182
217.706660	6980.925981	8.610394	-0.045433	4.507707
217.702727	6988.922594	8.615399	-0.045438	4.510206
217.780417	6997.011976	8.620403	-0.045458	4.512732
217.901368	7005.069572	8.625408	-0.045486	4.515248
218.041419	7012.999433	8.630413	-0.045518	4.517722
218.247524	7021.009326	8.635418	-0.045561	4.520220
218.219081	7029.002412	8.640423	-0.045562	4.522710
218.472738	7036.981840	8.645427	-0.045614	4.525196
218.658212	7045.025431	8.650432	-0.045654	4.527700
218.782098	7052.992663	8.655437	-0.045683	4.530179
218.818860	7061.106504	8.660442	-0.045695	4.532702
219.016394	7069.065085	8.665447	-0.045737	4.535176
219.354907	7077.104648	8.670451	-0.045806	4.537673
219.466267	7085.087765	8.675456	-0.045832	4.540152
219.607992	7093.093239	8.680461	-0.045864	4.542635
219.916022	7101.099207	8.685466	-0.045927	4.545118
219.678375	7109.147897	8.690471	-0.045888	4.547612
220.055008	7117.164451	8.695475	-0.045964	4.550096
220.416633	7125.247155	8.700480	-0.046036	4.552598
220.277070	7133.221799	8.705485	-0.046016	4.555065
220.446616	7141.242719	8.710490	-0.046053	4.557546
220.539994	7149.198697	8.715495	-0.046076	4.560005
220.671149	7157.237715	8.720499	-0.046106	4.562488
220.669044	7165.258443	8.725504	-0.046111	4.564964
220.843486	7173.257551	8.730509	-0.046149	4.567432
221.207239	7181.331262	8.735514	-0.046222	4.569922
221.339879	7189.357636	8.740519	-0.046252	4.572396
221.579308	7197.352585	8.745523	-0.046302	4.574859
221.772281	7205.401791	8.750528	-0.046343	4.577337
221.719661	7213.363790	8.755533	-0.046339	4.579787
221.890632	7221.434034	8.760538	-0.046376	4.582269
222.065253	7229.412199	8.765543	-0.046414	4.584722
222.145408	7237.448805	8.770547	-0.046435	4.587190
222.381332	7245.434531	8.775552	-0.046484	4.589642
222.386436	7253.506477	8.780557	-0.046491	4.592119
222.741803	7261.565907	8.785562	-0.046562	4.594591
222.704262	7269.516312	8.790567	-0.046561	4.597029
222.731939	7277.463710	8.795571	-0.046571	4.599463
223.027075	7285.560878	8.800576	-0.046632	4.601943
223.051713	7293.470949	8.805581	-0.046642	4.604364
223.346200	7301.618802	8.810586	-0.046702	4.606856
223.460396	7309.547577	8.815591	-0.046729	4.609280
223.608207	7317.603212	8.820595	-0.046762	4.611741
223.812198	7325.640712	8.825600	-0.046805	4.614196
223.759266	7333.662102	8.830605	-0.046801	4.616644
224.038740	7341.600807	8.835610	-0.046858	4.619066
224.126324	7349.677884	8.840615	-0.046880	4.621528
224.151399	7357.657819	8.845619	-0.046890	4.623960
224.307763	7365.709752	8.850624	-0.046925	4.626412
224.515073	7373.674777	8.855629	-0.046969	4.628837
224.564608	7381.761912	8.860634	-0.046984	4.631297
224.742909	7389.759077	8.865639	-0.047022	4.633729
224.748055	7397.766406	8.870643	-0.047029	4.636163
224.912025	7405.741230	8.875648	-0.047065	4.638585
225.064257	7413.738785	8.880653	-0.047098	4.641013
225.349758	7421.766616	8.885658	-0.047157	4.643449
225.288165	7429.800012	8.890663	-0.047151	4.645885
225.323448	7437.804893	8.895667	-0.047163	4.648312
225.456234	7445.819402	8.900672	-0.047193	4.650740
225.581996	7453.872172	8.905677	-0.047222	4.653178
226.086397	7461.896372	8.910682	-0.047322	4.655606
226.134998	7469.868714	8.915687	-0.047336	4.658017
226.320843	7477.903547	8.920691	-0.047376	4.660446
226.480637	7485.948756	8.925696	-0.047411	4.662877
226.349786	7493.896785	8.930701	-0.047393	4.665278
226.637299	7501.956123	8.935706	-0.047452	4.667710
226.626396	7509.923262	8.940711	-0.047455	4.670114
226.836305	7518.066390	8.945715	-0.047500	4.672569
227.232513	7526.103900	8.950720	-0.047579	4.674991
227.386298	7534.017027	8.955725	-0.047613	4.677374
227.453776	7542.037543	8.960730	-0.047631	4.679788
227.579497	7550.034524	8.965735	-0.047660	4.682195
227.763327	7558.008998	8.970739	-0.047699	4.684593
227.859442	7566.058820	8.975744	-0.047723	4.687012
227.706582	7574.037582	8.980749	-0.047700	4.689410
228.223748	7582.127410	8.985754	-0.047802	4.691838
228.071569	7590.106099	8.990759	-0.047779	4.694233
228.347318	7598.150923	8.995763	-0.047836	4.696645
228.598371	7606.133172	9.000768	-0.047888	4.699038
228.709394	7614.115507	9.005773	-0.047914	4.701430
228.789491	7622.130934	9.010778	-0.047934	4.703830
228.745338	7630.189234	9.015783	-0.047932	4.706243
229.199508	7638.163525	9.020787	-0.048022	4.708628
229.254168	7646.223572	9.025792	-0.048037	4.711038
228.964604	7654.247466	9.030797	-0.047989	4.713437
229.371676	7662.272579	9.035802	-0.048070	4.715833
229.388805	7670.224474	9.040807	-0.048079	4.718207
229.407779	7678.248420	9.045811	-0.048088	4.720602
229.742140	7686.313722	9.050816	-0.048155	4.723007
230.014936	7694.304170	9.055821	-0.048212	4.725388
230.136902	7702.363428	9.060826	-0.048240	4.727790
230.141080	7710.355502	9.065831	-0.048246	4.730170
230.301222	7718.383501	9.070835	-0.048281	4.732559
230.363778	7726.403144	9.075840	-0.048299	4.734945
230.297956	7734.409857	9.080845	-0.048292	4.737326
230.613410	7742.405474	9.085850	-0.048356	4.739702
230.706489	7750.447120	9.090855	-0.048379	4.742090
230.517849	7758.408960	9.095859	-0.048349	4.744455
230.933398	7766.489473	9.100864	-0.048432	4.746852
231.211341	7774.453792	9.105869	-0.048489	4.749213
231.472810	7782.484155	9.110874	-0.048543	4.751593
231.418135	7790.539368	9.115879	-0.048539	4.753980
231.630907	7798.560529	9.120883	-0.048584	4.756355
231.851844	7806.546851	9.125888	-0.048630	4.758718
231.761725	7814.496646	9.130893	-0.048619	4.761071
231.920501	7822.563137	9.135898	-0.048654	4.763456
232.027000	7830.550698	9.140903	-0.048679	4.765816
232.211681	7838.588684	9.145907	-0.048719	4.768190
232.454078	7846.618786	9.150912	-0.048770	4.770560
232.721861	7854.641667	9.155917	-0.048825	4.772927
232.877791	7862.690488	9.160922	-0.048860	4.775301
232.701820	7870.655361	9.165927	-0.048832	4.777650
232.938108	7878.671962	9.170931	-0.048882	4.780011
233.251480	7886.693665	9.175936	-0.048946	4.782373
233.332737	7894.662188	9.180941	-0.048966	4.784718
233.356167	7902.730434	9.185946	-0.048976	4.787092
233.542949	7910.759344	9.190951	-0.049016	4.789453
233.629933	7918.783434	9.195955	-0.049038	4.791811
233.599731	7926.800259	9.200960	-0.049038	4.794167
233.757066	7934.776983	9.205965	-0.049072	4.796509
233.705776	7942.733299	9.210970	-0.049068	4.798844
233.701528	7950.789985	9.215975	-0.049073	4.801208
233.914213	7958.746393	9.220979	-0.049118	4.803540
234.016001	7966.822247	9.225984	-0.049143	4.805906
233.972995	7974.807126	9.230989	-0.049140	4.808246
234.235210	7982.871103	9.235994	-0.049194	4.810606
234.322431	7990.288661	9.240999	-0.049216	4.812776
234.590222	7994.813461	9.246003	-0.049269	4.814099

234.562171	7997.230659	9.251008	-0.049265	4.814806
234.719858	7998.504635	9.256013	-0.049296	4.815178
234.885366	7998.981339	9.261018	-0.049327	4.815316
234.902187	7999.813304	9.266023	-0.049331	4.815559
234.853447	7999.847766	9.271027	-0.049322	4.815570
235.027844	7999.835671	9.276032	-0.049355	4.815565
234.955138	7999.801415	9.281037	-0.049342	4.815556
235.083803	7999.853705	9.286042	-0.049366	4.815570
235.149079	7999.805674	9.291047	-0.049378	4.815556
235.226863	7999.829378	9.296051	-0.049393	4.815562
235.254842	7999.838395	9.301056	-0.049398	4.815565
235.381052	7999.806300	9.306061	-0.049422	4.815555
235.495669	7999.838077	9.311066	-0.049444	4.815564
235.448841	7999.820255	9.316071	-0.049435	4.815559
235.369526	7999.847815	9.321075	-0.049421	4.815567
235.604561	7999.838841	9.326080	-0.049465	4.815563
235.531028	7999.778947	9.331085	-0.049451	4.815546
235.542039	7999.807973	9.336090	-0.049454	4.815555
235.953151	7999.822144	9.341095	-0.049530	4.815557
235.842052	7999.806481	9.346099	-0.049510	4.815553
235.879428	7999.840207	9.351104	-0.049517	4.815562
235.832489	7999.824519	9.356109	-0.049509	4.815558
235.797188	7999.859200	9.361114	-0.049502	4.815568
235.904461	7999.825730	9.366119	-0.049522	4.815558
235.801651	7999.829420	9.371123	-0.049504	4.815560
235.888963	7999.832994	9.376128	-0.049520	4.815560
235.829134	7999.794676	9.381133	-0.049509	4.815549
235.947122	7999.813695	9.386138	-0.049531	4.815554
236.045769	7999.804642	9.391143	-0.049550	4.815551
236.232910	7999.834394	9.396147	-0.049585	4.815559
236.333675	7999.848864	9.401152	-0.049604	4.815563
236.241538	7999.827103	9.406157	-0.049587	4.815557
236.392179	7999.858398	9.411162	-0.049615	4.815565
236.311483	7999.838958	9.416167	-0.049601	4.815560
236.355944	7999.869597	9.421171	-0.049609	4.815569
236.312881	7999.876392	9.426176	-0.049601	4.815571
236.375231	7999.848599	9.431181	-0.049613	4.815562
236.368870	7999.848517	9.436186	-0.049612	4.815562
236.278080	7999.831048	9.441191	-0.049596	4.815558
236.323465	7999.822197	9.446195	-0.049604	4.815555
236.554459	7999.867610	9.451200	-0.049648	4.815567
236.289711	7999.835571	9.456205	-0.049599	4.815559
236.614692	7999.854751	9.461210	-0.049659	4.815563
236.519022	7999.839338	9.466215	-0.049642	4.815559
236.293465	7999.845305	9.471219	-0.049600	4.815562
236.423878	7999.839971	9.476224	-0.049625	4.815560
236.501579	7999.804953	9.481229	-0.049639	4.815549
236.295089	7999.834718	9.486234	-0.049601	4.815559
236.354505	7999.829298	9.491239	-0.049612	4.815557
236.687109	7999.833655	9.496243	-0.049675	4.815557
236.547395	7999.842083	9.501248	-0.049649	4.815560
236.635297	7999.826449	9.506253	-0.049665	4.815555
236.871613	7999.818565	9.511258	-0.049710	4.815551
236.812798	7999.812292	9.516263	-0.049699	4.815550
236.519885	7999.855601	9.521267	-0.049645	4.815564
236.664594	7999.845161	9.526272	-0.049672	4.815560
236.759166	7999.825364	9.531277	-0.049690	4.815554
236.916809	7999.877061	9.536282	-0.049719	4.815568
236.715914	7999.850329	9.541287	-0.049682	4.815561
237.026778	7999.860739	9.546291	-0.049740	4.815563
237.042677	7999.848206	9.551296	-0.049743	4.815559
236.861613	7999.829270	9.556301	-0.049710	4.815554
236.776489	7999.847127	9.561306	-0.049694	4.815560
237.026236	7999.826649	9.566311	-0.049741	4.815553
237.144168	7999.861685	9.571315	-0.049763	4.815562
237.089938	7999.848012	9.576320	-0.049753	4.815559
236.995223	7999.836885	9.581325	-0.049736	4.815556
237.098799	7999.856740	9.586330	-0.049756	4.815561
237.060029	7999.827304	9.591335	-0.049749	4.815553
237.043975	7999.819590	9.596339	-0.049746	4.815551
237.154845	7999.851309	9.601344	-0.049767	4.815559
236.940956	7999.824365	9.606349	-0.049727	4.815552
237.068701	7999.855290	9.611354	-0.049751	4.815561
237.096635	7999.832275	9.616359	-0.049757	4.815554
237.038442	7999.798252	9.621363	-0.049746	4.815544
237.150663	7999.855617	9.626368	-0.049767	4.815561
237.226062	7999.782125	9.631373	-0.049781	4.815539
237.112366	7999.789908	9.636378	-0.049760	4.815542
237.001884	7999.777457	9.641383	-0.049740	4.815538
237.082818	7999.814027	9.646387	-0.049755	4.815549
237.127377	7999.854277	9.651392	-0.049764	4.815560
237.050946	7999.791130	9.656397	-0.049750	4.815542
237.198470	7999.829850	9.661402	-0.049778	4.815553
237.304684	7999.821988	9.666407	-0.049798	4.815550
237.133317	7999.832037	9.671411	-0.049766	4.815554
237.248008	7999.827516	9.676416	-0.049788	4.815552
237.258436	7999.903513	9.681421	-0.049790	4.815574
237.284608	7999.875132	9.686426	-0.049795	4.815566
237.197590	7999.827828	9.691431	-0.049779	4.815552
237.160968	7999.865691	9.696435	-0.049772	4.815563
237.315883	7999.828725	9.701440	-0.049802	4.815552
237.238566	7999.869130	9.706445	-0.049787	4.815564
237.445436	7999.815924	9.711450	-0.049826	4.815547
237.591129	7999.920814	9.716455	-0.049854	4.815577
237.471463	7999.830270	9.721459	-0.049831	4.815552
237.656612	7999.874941	9.726464	-0.049866	4.815564
237.406145	7999.797220	9.731469	-0.049820	4.815542
237.479599	7999.860362	9.736474	-0.049834	4.815560
237.451282	7999.928256	9.741479	-0.049829	4.815580
237.559547	7999.836078	9.746483	-0.049849	4.815553
237.508988	7999.851293	9.751488	-0.049840	4.815557
237.447539	7999.819352	9.756493	-0.049829	4.815548
237.308880	7999.833136	9.761498	-0.049803	4.815553
237.346987	7999.927735	9.766503	-0.049811	4.815581
237.374442	7999.832108	9.771507	-0.049816	4.815552
237.465234	7999.874178	9.776512	-0.049833	4.815564
237.336246	7999.827259	9.781517	-0.049809	4.815551
237.303976	7999.834230	9.786522	-0.049803	4.815553
237.382782	7999.902798	9.791527	-0.049818	4.815573
237.422542	7999.884246	9.796531	-0.049826	4.815567
237.328990	7999.832565	9.801536	-0.049809	4.815553
237.172054	7999.828968	9.806541	-0.049780	4.815552
237.424499	7999.838430	9.811546	-0.049827	4.815554
237.503997	7999.933702	9.816551	-0.049842	4.815582
237.501599	7999.834387	9.821555	-0.049842	4.815552
237.633071	7999.878186	9.826560	-0.049867	4.815565
237.740108	7999.837238	9.831565	-0.049887	4.815552
237.895094	7999.862200	9.836570	-0.049916	4.815559
237.616989	7999.836347	9.841575	-0.049864	4.815552
237.553366	7999.856688	9.846579	-0.049853	4.815559
237.769316	7999.956315	9.851584	-0.049893	4.815587
237.635241	7999.858062	9.856589	-0.049869	4.815559
237.588305	7999.871200	9.861594	-0.049860	4.815563
237.765120	7999.827116	9.866599	-0.049893	4.815549
237.785192	7999.879781	9.871603	-0.049897	4.815564
237.714772	7999.895741	9.876608	-0.049884	4.815569
237.592191	7999.852129	9.881613	-0.049862	4.815557
237.638179	7999.880659	9.886618	-0.049871	4.815565
237.719615	7999.848904	9.891623	-0.049886	4.815556
237.702726	7999.825161	9.896627	-0.049883	4.815549
238.048507	7999.844683	9.901632	-0.049948	4.815553
237.873259	7999.855736	9.906637	-0.049915	4.815557
237.808857	7999.873929	9.911642	-0.049904	4.815562
237.780637	7999.846799	9.916647	-0.049899	4.815555
237.897368	7999.940542	9.921651	-0.049921	4.815582
237.821929	7999.871002	9.926656	-0.049907	4.815562
237.688967	7999.836831	9.931661	-0.049882	4.815552
237.742050	7999.829173	9.936666	-0.049892	4.815550
237.883938	7999.943612	9.941671	-0.049919	4.815582
237.770469	7999.871318	9.946675	-0.049898	4.815562
238.007514	7999.879464	9.951680	-0.049943	4.815563
237.763963	7999.861646	9.956685	-0.049897	4.815559
237.733089	7999.829133	9.961690	-0.049892	4.815550
237.677412	7999.952105	9.966695	-0.049882	4.815586
237.828736	7999.832866	9.971699	-0.049910	4.815550
238.021969	7999.843502	9.976704	-0.049946	4.815552
237.831774	7999.895953	9.981709	-0.049911	4.815569
238.114065	7999.858922	9.986714	-0.049964	4.815557
237.985754	7999.917718	9.991719	-0.049940	4.815574
237.901731	7999.853377	9.996723	-0.049925	4.815556
238.080346	7999.878724	10.001728	-0.049959	4.815562
237.970679	7999.812899	10.006733	-0.049938	4.815544
237.812591	7999.943816	10.011738	-0.049909	4.815583
237.828283	7999.847998	10.016743	-0.049912	4.815555
237.766482	7999.819254	10.021747	-0.049901	4.815547
237.759201	7999.857594	10.026752	-0.049900	4.815558
237.629637	7999.922776	10.031757	-0.049876	4.815577
237.831417	7999.894045	10.036762	-0.049914	4.815568
237.808911	7999.865940	10.041767	-0.049910	4.815560
237.811151	7999.863862	10.046771	-0.049911	4.815559
237.976940	7999.870849	10.051776	-0.049942	4.815561
237.967477	7999.836549	10.056781	-0.049940	4.815551
238.004756	7999.838244	10.061786	-0.049947	4.815551
237.898058	7999.860021	10.066791	-0.049928	4.815558
237.940831	7999.848993	10.071795	-0.049936	4.815554
237.831610	7999.835493	10.076800	-0.049916	4.815551
238.056103	7999.859451	10.081805	-0.049958	4.815557
238.094603	7999.946584	10.086810	-0.049965	4.815582
238.020253	7999.850368	10.091815	-0.049952	4.815554
238.086757	7999.855742	10.096819	-0.049964	4.815556
238.049379	7999.840207	10.101824	-0.049958	4.815551
237.983944	7999.831691	10.106829	-0.049946	4.815549
237.988841	7999.863823	10.111834	-0.049947	4.815558
238.080692	7999.925130	10.116839	-0.049964	4.815576
238.000261	7999.867254	10.121843	-0.049949	4.815559
237.983788	7999.859534	10.126848	-0.049947	4.815557
237.854093	7999.820076	10.131853	-0.049923	4.815546
238.308583	7999.895821	10.136858	-0.050008	4.815566
238.387433	7999.936630	10.141863	-0.050023	4.815578
238.132120	7999.813982	10.146867	-0.049975	4.815543
238.207156	7999.844052	10.151872	-0.049989	4.815552
238.138743	7999.937989	10.156877	-0.049977	4.815579
238.345036	7999.877300	10.161882	-0.050016	4.815561
238.103005	7999.874454	10.166887	-0.049971	4.815561
238.077139	7999.840955	10.171891	-0.049966	4.815551
238.358285	7999.883986	10.176896	-0.050019	4.815562
238.273659	7999.842057	10.181901	-0.050003	4.815551
238.382141	7999.844910	10.186906	-0.050024	4.815551
238.335392	7999.939200	10.191911	-0.050015	4.815579
238.162393	7999.816822	10.196915	-0.049983	4.815544
238.217183	7999.852969	10.201920	-0.049994	4.815554
238.158238	7999.906486	10.206925	-0.049983	4.815570
238.342025	7999.831551	10.211930	-0.050017	4.815547
238.151878	7999.840226	10.216935	-0.049982	4.815551
238.246027	7999.843913	10.221939	-0.050000	4.815551
238.224274	7999.870274	10.226944	-0.049996	4.815559
238.000925	7999.933931	10.231949	-0.049955	4.815579
238.123463	7999.865474	10.236954	-0.049978	4.815558
238.215149	7999.824277	10.241959	-0.049995	4.815546
238.060335	7999.925351	10.246963	-0.049967	4.815576
238.389428	7999.839965	10.251968	-0.050028	4.815549
238.312074	7999.831255	10.256973	-0.050014	4.815547
238.420328	7999.891762	10.261978	-0.050034	4.815564
238.321219	7999.870952	10.266983	-0.050016	4.815559
238.374269	7999.865429	10.271987	-0.050026	4.815557
238.612115	7999.936586	10.276992	-0.050071	4.815577
238.456133	7999.899903	10.281997	-0.050042	4.815567
238.642382	7999.869853	10.287002	-0.050077	4.815557
238.330095	7999.872270	10.292007	-0.050019	4.815559
238.157492	7999.875892	10.297011	-0.049987	4.815561
238.396211	7999.892607	10.302016	-0.050032	4.815565
238.431544	7999.881458	10.307021	-0.050039	4.815561
238.533297	7999.898082	10.312026	-0.050058	4.815566
238.414608	7999.857734	10.317031	-0.050036	4.815554
238.409078	7999.859801	10.322035	-0.050035	4.815555
238.512691	7999.868981	10.327040	-0.050055	4.815557
238.457687	7999.859566	10.332045	-0.050045	4.815555
238.478141	7999.967762	10.337050	-0.050049	4.815586
238.628152	7999.871990	10.342055	-0.050077	4.815557
238.415162	7999.850396	10.347059	-0.050038	4.815552
238.484607	7999.876105	10.352064	-0.050051	4.815559
238.599485	7999.848097	10.357069	-0.050072	4.815551
238.513460	7999.861668	10.362074	-0.050057	4.815555
238.506238	7999.830607	10.367079	-0.050056	4.815546
238.358418	7999.916847	10.372083	-0.050028	4.815572
238.559805	7999.843266	10.377088	-0.050066	4.815549
238.466261	7999.841766	10.382093	-0.050049	4.815549
238.287934	7999.909359	10.387098	-0.050016	4.815570
238.335209	7999.877049	10.392103	-0.050025	4.815560
238.249475	7999.852186	10.397107	-0.050009	4.815553
238.376235	7999.857471	10.402112	-0.050033	4.815554
238.444876	7999.851134	10.407117	-0.050046	4.815552
238.236092	7999.862709	10.412122	-0.050007	4.815557
238.442162	7999.873555	10.417127	-0.050046	4.815559
238.473416	7999.860204	10.422131	-0.050052	4.815555
238.706591	7999.881101	10.427136	-0.050096	4.815560
238.429284	7999.837106	10.432141	-0.050044	4.815548
238.359504	7999.939564	10.437146	-0.050032	4.815578
238.691154	7999.857423	10.442151	-0.050094	4.815553
238.458781	7999.856869	10.447155	-0.050051	4.815554
238.609635	7999.902053	10.452160	-0.050079	4.815566
238.425993	7999.878801	10.457165	-0.050045	4.815560
238.640636	7999.910073	10.462170	-0.050085	4.815568
238.428061	7999.882080	10.467175	-0.050046	4.815561
238.316340	7999.849320	10.472179	-0.050025	4.815552
238.691593	7999.876798	10.477184	-0.050095	4.815558
238.465077	7999.849645	10.482189	-0.050053	4.815552
238.419560	7999.936481	10.487194	-0.050045	4.815577
238.466528	7999.842237	10.492199	-0.050054	4.815549
238.521123	7999.859162	10.497203	-0.050065	4.815554
238.580580	7999.886844	10.502208	-0.050076	4.815562
238.440780	7999.882456	10.507213	-0.050050	4.815561
238.446560	7999.909265	10.512218	-0.050051	4.815569
238.515956	7999.859163	10.517223	-0.050065	4.815554
238.657645	7999.858285	10.522227	-0.050091	4.815553
238.580919	7999.894430	10.527232	-0.050077	4.815564
238.611635	7999.952609	10.532237	-0.050083	4.815581
238.564567	7999.876055	10.537242	-0.050075	4.815559
238.563970	7999.868592	10.542247	-0.050075	4.815557
238.464180	7999.840297	10.547251	-0.050056	4.815549
238.434234	7999.886812	10.552256	-0.050051	4.815562
238.447693	7999.867833	10.557261	-0.050054	4.815557
238.652288	7999.880790	10.562266	-0.050092	4.815560
238.660695	7999.957826	10.567271	-0.050094	4.815582
238.554599	7999.845076	10.572275	-0.050074	4.815550
238.587679	7999.886210	10.577280	-0.050081	4.815562
238.653138	7999.830705	10.582285	-0.050093	4.815545
238.362673	7999.840952	10.587290	-0.050039	4.815549
238.482113	7999.931538	10.592295	-0.050062	4.815575
238.582190	7999.858444	10.597299	-0.050081	4.815553
238.645984	7999.881925	10.602304	-0.050093	4.815560
238.493172	7999.852768	10.607309	-0.050065	4.815552
238.542562	7999.882422	10.612314	-0.050074	4.815561
238.538027	7999.854608	10.617319	-0.050074	4.815552
238.691490	7999.932935	10.622323	-0.050102	4.815575
238.750681	7999.894412	10.627328	-0.050114	4.815563
238.637160	7999.874435	10.632333	-0.050093	4.815558
238.400513	7999.874879	10.637338	-0.050049	4.815559
238.712672	7999.844741	10.642343	-0.050107	4.815549
238.706300	7999.877758	10.647347	-0.050106	4.815558
238.661180	7999.903740	10.652352	-0.050098	4.815566
238.547539	7999.858135	10.657357	-0.050077	4.815553
238.778859	7999.975100	10.662362	-0.050121	4.815587
238.941175	7999.866715	10.667367	-0.050151	4.815554
238.793074	7999.861124	10.672371	-0.050124	4.815553
238.878099	7999.896696	10.677376	-0.050140	4.815563
238.730889	7999.861223	10.682381	-0.050113	4.815553
238.751893	7999.887212	10.687386	-0.050117	4.815561
238.851955	7999.878183	10.692391	-0.050136	4.815558
238.738901	7999.829384	10.697395	-0.050115	4.815544
238.699237	7999.905639	10.702400	-0.050108	4.815567
238.424265	7999.845666	10.707405	-0.050057	4.815550
238.563622	7999.882121	10.712410	-0.050083	4.815560
238.606006	7999.952235	10.717415	-0.050091	4.815581
238.506665	7999.825714	10.722419	-0.050073	4.815544
238.728164	7999.881657	10.727424	-0.050114	4.815559
238.605156	7999.862594	10.732429	-0.050092	4.815554
238.763005	7999.907892	10.737434	-0.050121	4.815567
238.681908	7999.898052	10.742439	-0.050106	4.815564
238.686430	7999.887470	10.747443	-0.050108	4.815561
238.792607	7999.890285	10.752448	-0.050128	4.815562
238.629810	7999.936775	10.757453	-0.050098	4.815576
238.802669	7999.877678	10.762458	-0.050130	4.815558
238.833231	7999.897416	10.767463	-0.050136	4.815563
238.568060	7999.858957	10.772467	-0.050087	4.815553
238.832279	7999.872885	10.777472	-0.050136	4.815556
238.901125	7999.860145	10.782477	-0.050149	4.815552
238.836858	7999.892221	10.787482	-0.050138	4.815562
238.705501	7999.885835	10.792487	-0.050113	4.815561
238.756676	7999.869605	10.797491	-0.050123	4.815556
238.746513	7999.885477	10.802496	-0.050121	4.815560
238.703472	7999.855969	10.807501	-0.050114	4.815552
238.721359	7999.881907	10.812506	-0.050117	4.815559
238.870884	7999.947358	10.817511	-0.050145	4.815578
238.900884	7999.850701	10.822515	-0.050151	4.815549
238.746231	7999.868494	10.827520	-0.050123	4.815555
238.868380	7999.851282	10.832525	-0.050146	4.815550
238.961552	7999.827193	10.837530	-0.050163	4.815542
238.775197	7999.957653	10.842535	-0.050129	4.815581
238.782496	7999.849949	10.847539	-0.050130	4.815550
238.978943	7999.885198	10.852544	-0.050167	4.815559
238.749052	7999.849448	10.857549	-0.050125	4.815550
238.662660	7999.877961	10.862554	-0.050109	4.815558
238.897610	7999.886075	10.867559	-0.050153	4.815560
239.046809	7999.879980	10.872563	-0.050181	4.815557
238.994002	7999.909040	10.877568	-0.050171	4.815566
239.058641	7999.878080	10.882573	-0.050183	4.815557
239.015684	7999.899825	10.887578	-0.050176	4.815563
238.976738	7999.905620	10.892583	-0.050169	4.815565
238.841028	7999.892756	10.897587	-0.050144	4.815562
238.951943	7999.904191	10.902592	-0.050165	4.815565
238.814145	7999.874209	10.907597	-0.050139	4.815557
238.760106	7999.888300	10.912602	-0.050129	4.815561
239.100715	7999.955792	10.917607	-0.050193	4.815579
239.074216	7999.878503	10.922611	-0.050188	4.815557
239.051059	7999.894164	10.927616	-0.050184	4.815561
238.982256	7999.889863	10.932621	-0.050172	4.815560
239.089051	7999.903366	10.937626	-0.050192	4.815564
238.911808	7999.893030	10.942631	-0.050159	4.815562
238.961837	7999.889594	10.947635	-0.050169	4.815560
238.887784	7999.925783	10.952640	-0.050155	4.815571
238.797922	7999.852803	10.957645	-0.050139	4.815550
238.867940	7999.879589	10.962650	-0.050152	4.815558
238.891418	7999.902415	10.967655	-0.050156	4.815564
238.757834	7999.888518	10.972659	-0.050132	4.815561
238.868708	7999.926646	10.977664	-0.050153	4.815572
238.944047	7999.892657	10.982669	-0.050167	4.815561
239.051770	7999.902972	10.987674	-0.050187	4.815564
238.983221	7999.885862	10.992679	-0.050175	4.815559
239.050305	7999.875229	10.997683	-0.050187	4.815556
239.193371	7999.914949	11.002688	-0.050214	4.815567
238.918444	7999.879533	11.007693	-0.050163	4.815557
239.090304	7999.911179	11.012698	-0.050196	4.815566
239.123085	7999.880769	11.017703	-0.050202	4.815557
238.951250	7999.897215	11.022707	-0.050170	4.815562
239.050702	7999.912734	11.027712	-0.050189	4.815567
239.176414	7999.895581	11.032717	-0.050213	4.815561
239.068661	7999.964322	11.037722	-0.050193	4.815582
239.124105	7999.880891	11.042727	-0.050203	4.815557
238.910635	7999.816579	11.047731	-0.050164	4.815539
239.064884	7999.872496	11.052736	-0.050193	4.815555
238.921207	7999.868045	11.057741	-0.050166	4.815554
238.896351	7999.912508	11.062746	-0.050162	4.815567
238.901726	7999.905142	11.067751	-0.050163	4.815565
239.062965	7999.894973	11.072755	-0.050193	4.815561
238.993212	7999.907741	11.077760	-0.050181	4.815565
238.961811	7999.898709	11.082765	-0.050175	4.815563
239.344222	7999.946594	11.087770	-0.050247	4.815575
239.204714	7999.873873	11.092775	-0.050221	4.815554
239.143639	7999.877172	11.097779	-0.050210	4.815556
239.191494	7999.896123	11.102784	-0.050219	4.815561
239.318273	7999.866174	11.107789	-0.050243	4.815552
239.045146	7999.885243	11.112794	-0.050192	4.815558
239.174193	7999.873482	11.117799	-0.050216	4.815554
239.194415	7999.905866	11.122803	-0.050220	4.815564
239.301699	7999.831821	11.127808	-0.050241	4.815542
239.058040	7999.927180	11.132813	-0.050195	4.815571
238.970203	7999.874520	11.137818	-0.050179	4.815556
239.255050	7999.908005	11.142823	-0.050233	4.815564
239.208510	7999.837864	11.147827	-0.050224	4.815544
239.316783	7999.870612	11.152832	-0.050245	4.815553
239.091623	7999.957730	11.157837	-0.050203	4.815579
239.006683	7999.863475	11.162842	-0.050187	4.815552
239.133211	7999.852741	11.167847	-0.050211	4.815548
239.122015	7999.856851	11.172851	-0.050209	4.815550
239.247473	7999.904827	11.177856	-0.050233	4.815563
239.113556	7999.881314	11.182861	-0.050208	4.815557
239.111517	7999.896251	11.187866	-0.050208	4.815561
239.110130	7999.882369	11.192871	-0.050208	4.815557
239.206210	7999.873275	11.197875	-0.050226	4.815554
238.988852	7999.916742	11.202880	-0.050186	4.815568
239.040869	7999.877035	11.207885	-0.050196	4.815556
239.001276	7999.888157	11.212890	-0.050189	4.815559
238.960463	7999.970800	11.217895	-0.050181	4.815584
238.867232	7999.834767	11.222899	-0.050164	4.815544
239.245355	7999.872971	11.227904	-0.050235	4.815554
239.208902	7999.855316	11.232909	-0.050228	4.815549
239.339240	7999.901235	11.237914	-0.050253	4.815562
239.297932	7999.908059	11.242919	-0.050245	4.815564
239.146059	7999.917355	11.247923	-0.050217	4.815567
239.171902	7999.878289	11.252928	-0.050222	4.815556
239.065196	7999.887253	11.257933	-0.050203	4.815559
239.177518	7999.900846	11.262938	-0.050224	4.815562
239.156520	7999.890916	11.267943	-0.050220	4.815559
239.265676	7999.903391	11.272947	-0.050241	4.815562
239.332727	7999.917316	11.277952	-0.050254	4.815566
238.963659	7999.877165	11.282957	-0.050185	4.815556
239.095992	7999.884678	11.287962	-0.050210	4.815558
239.028038	7999.884661	11.292967	-0.050198	4.815558
239.223992	7999.866515	11.297971	-0.050234	4.815552
239.217201	7999.899526	11.302976	-0.050233	4.815562
239.185055	7999.848839	11.307981	-0.050228	4.815547
239.160285	7999.898643	11.312986	-0.050223	4.815562
239.264059	7999.884335	11.317991	-0.050243	4.815557
239.262111	7999.896070	11.322995	-0.050243	4.815560
239.359190	7999.975618	11.328000	-0.050261	4.815583
239.353301	7999.878377	11.333005	-0.050260	4.815555
239.349324	7999.870859	11.338010	-0.050260	4.815552
239.210055	7999.879292	11.343015	-0.050234	4.815556
239.332006	7999.873823	11.348019	-0.050257	4.815553
239.192603	7999.920694	11.353024	-0.050231	4.815568
239.156583	7999.876350	11.358029	-0.050225	4.815555
239.104692	7999.853105	11.363034	-0.050215	4.815548
239.331080	7999.972128	11.368039	-0.050258	4.815582
239.102737	7999.853115	11.373043	-0.050215	4.815548
239.192482	7999.865274	11.378048	-0.050232	4.815552
239.060922	7999.841800	11.383053	-0.050208	4.815545
239.107617	7999.847919	11.388058	-0.050217	4.815547
239.382648	7999.923955	11.393063	-0.050269	4.815568
239.326461	7999.833370	11.398067	-0.050258	4.815542
239.425917	7999.877719	11.403072	-0.050277	4.815554
239.326628	7999.840889	11.408077	-0.050259	4.815544
239.431832	7999.904552	11.413082	-0.050279	4.815562
239.395188	7999.881554	11.418087	-0.050272	4.815555
239.103903	7999.953716	11.423091	-0.050218	4.815578
239.398083	7999.902999	11.428096	-0.050273	4.815562
239.546878	7999.862730	11.433101	-0.050301	4.815549
239.359636	7999.894942	11.438106	-0.050266	4.815559
239.349424	7999.887323	11.443111	-0.050265	4.815557
239.250963	7999.868658	11.448115	-0.050247	4.815552
239.206687	7999.892517	11.453120	-0.050239	4.815559
239.206232	7999.859431	11.458125	-0.050239	4.815550
239.126846	7999.877380	11.463130	-0.050224	4.815555
239.125137	7999.888051	11.468135	-0.050224	4.815558
239.125542	7999.930790	11.473139	-0.050225	4.815571
239.471596	7999.894798	11.478144	-0.050289	4.815559
239.281861	7999.860767	11.483149	-0.050254	4.815550
239.149830	7999.867183	11.488154	-0.050230	4.815552
239.515468	7999.864610	11.493159	-0.050298	4.815550
239.462215	7999.908611	11.498163	-0.050288	4.815563
239.447598	7999.894513	11.503168	-0.050286	4.815559
239.397163	7999.874494	11.508173	-0.050277	4.815553
239.339670	7999.887461	11.513178	-0.050266	4.815557
239.434668	7999.887960	11.518183	-0.050284	4.815557
239.094739	7999.846148	11.523187	-0.050221	4.815546
239.156209	7999.889879	11.528192	-0.050233	4.815559
239.143142	7999.852316	11.533197	-0.050231	4.815548
239.272256	7999.911029	11.538202	-0.050255	4.815564
239.398179	7999.946200	11.543207	-0.050279	4.815574
239.219487	7999.855757	11.548211	-0.050246	4.815548
239.188453	7999.899052	11.553216	-0.050240	4.815561
239.160079	7999.885798	11.558221	-0.050235	4.815557
239.337953	7999.898323	11.563226	-0.050268	4.815560
239.394678	7999.898200	11.568231	-0.050279	4.815560
239.296527	7999.850710	11.573235	-0.050261	4.815547
239.481339	7999.901787	11.578240	-0.050296	4.815561
239.228406	7999.869932	11.583245	-0.050249	4.815552
239.197615	7999.888672	11.588250	-0.050244	4.815558
239.306808	7999.897944	11.593255	-0.050264	4.815560
239.165470	7999.854023	11.598259	-0.050238	4.815548
239.289776	7999.909455	11.603264	-0.050261	4.815564
239.106699	7999.964157	11.608269	-0.050228	4.815581
239.300298	7999.855212	11.613274	-0.050264	4.815548
239.038226	7999.866987	11.618279	-0.050215	4.815552
239.058485	7999.858795	11.623283	-0.050219	4.815550
239.138431	7999.893218	11.628288	-0.050234	4.815560
239.107853	7999.843624	11.633293	-0.050229	4.815545
239.197261	7999.929454	11.638298	-0.050246	4.815570
239.207785	7999.865580	11.643303	-0.050248	4.815551
239.351480	7999.852990	11.648307	-0.050275	4.815547
239.183829	7999.909011	11.653312	-0.050244	4.815564
239.390190	7999.859001	11.658317	-0.050283	4.815548
239.289614	7999.890487	11.663322	-0.050264	4.815558
239.287265	7999.866979	11.668327	-0.050264	4.815551
239.271320	7999.843250	11.673331	-0.050261	4.815544
239.340702	7999.887111	11.678336	-0.050275	4.815557
239.364980	7999.853358	11.683341	-0.050279	4.815547
239.159886	7999.955752	11.688346	-0.050241	4.815578
239.326933	7999.880544	11.693351	-0.050273	4.815555
239.491892	7999.862961	11.698355	-0.050304	4.815549
239.267903	7999.892439	11.703360	-0.050262	4.815559
239.264652	7999.849697	11.708365	-0.050262	4.815546
239.228139	7999.916393	11.713370	-0.050255	4.815566
239.268853	7999.857282	11.718375	-0.050263	4.815548
239.117380	7999.827077	11.723379	-0.050235	4.815540
239.349089	7999.885324	11.728384	-0.050279	4.815556
239.357129	7999.872663	11.733389	-0.050280	4.815552
239.271081	7999.885165	11.738394	-0.050265	4.815557
239.339022	7999.943951	11.743399	-0.050277	4.815573
239.309001	7999.824962	11.748403	-0.050272	4.815539
239.545108	7999.891822	11.753408	-0.050316	4.815557
239.626345	7999.856861	11.758413	-0.050332	4.815547
239.667326	7999.871430	11.763418	-0.050340	4.815551
239.564901	7999.884734	11.768423	-0.050321	4.815555
239.297751	7999.910306	11.773427	-0.050271	4.815564
239.264650	7999.885230	11.778432	-0.050265	4.815557
239.195181	7999.846750	11.783437	-0.050253	4.815546
239.397972	7999.828714	11.788442	-0.050291	4.815539
239.432943	7999.958505	11.793447	-0.050297	4.815577
239.453021	7999.837127	11.798451	-0.050301	4.815542
239.367643	7999.852843	11.803456	-0.050286	4.815547
239.275608	7999.959212	11.808461	-0.050269	4.815578
239.327565	7999.839420	11.813466	-0.050279	4.815543
239.516221	7999.840375	11.818471	-0.050314	4.815542
239.617915	7999.918931	11.823475	-0.050333	4.815565
239.670796	7999.901660	11.828480	-0.050343	4.815559
239.576166	7999.843550	11.833485	-0.050326	4.815543
239.443829	7999.862773	11.838490	-0.050302	4.815549
239.648712	7999.898161	11.843495	-0.050340	4.815558
239.713176	7999.902435	11.848499	-0.050352	4.815559
239.500444	7999.911808	11.853504	-0.050313	4.815563
239.413273	7999.938173	11.858509	-0.050297	4.815571
239.736936	7999.854835	11.863514	-0.050357	4.815545
239.741709	7999.862408	11.868519	-0.050358	4.815547
239.357286	7999.830549	11.873523	-0.050287	4.815540
239.430388	7999.881945	11.878528	-0.050301	4.815555
239.525813	7999.865366	11.883533	-0.050319	4.815549
239.429178	7999.856341	11.888538	-0.050301	4.815547
239.471551	7999.967032	11.893543	-0.050309	4.815579
239.494414	7999.858512	11.898547	-0.050314	4.815547
239.609936	7999.871091	11.903552	-0.050336	4.815551
239.468867	7999.869885	11.908557	-0.050310	4.815551
239.478801	7999.885016	11.913562	-0.050312	4.815555
239.540728	7999.895655	11.918567	-0.050323	4.815558
239.675579	7999.834872	11.923571	-0.050349	4.815540
239.727016	7999.908339	11.928576	-0.050359	4.815561
239.625407	7999.890690	11.933581	-0.050340	4.815556
239.358354	7999.940823	11.938586	-0.050291	4.815572
239.541554	7999.898978	11.943591	-0.050325	4.815559
239.492260	7999.867232	11.948595	-0.050316	4.815550
239.758305	7999.905751	11.953600	-0.050366	4.815560
239.576294	7999.872913	11.958605	-0.050332	4.815551
239.662154	7999.887144	11.963610	-0.050348	4.815555
239.806597	7999.862821	11.968615	-0.050375	4.815547
239.601323	7999.859502	11.973619	-0.050337	4.815547
239.498128	7999.875997	11.978624	-0.050318	4.815552
239.631131	7999.961469	11.983629	-0.050344	4.815577
239.468625	7999.879830	11.988634	-0.050313	4.815554
239.594053	7999.898977	11.993639	-0.050337	4.815559
239.393319	7999.878648	11.998643	-0.050300	4.815554
239.771427	7999.891228	12.003648	-0.050371	4.815556
239.385739	7999.861482	12.008653	-0.050299	4.815549
239.375475	7999.883760	12.013658	-0.050297	4.815555
239.600006	7999.911993	12.018663	-0.050339	4.815562
239.469296	7999.862905	12.023667	-0.050315	4.815549
239.508525	7999.913751	12.028672	-0.050323	4.815563
239.428963	7999.892189	12.033677	-0.050308	4.815557
239.559499	7999.903945	12.038682	-0.050333	4.815560
239.408262	7999.881217	12.043687	-0.050305	4.815554
239.491536	7999.863373	12.048691	-0.050321	4.815549
239.541723	7999.882363	12.053696	-0.050330	4.815554
239.542671	7999.889875	12.058701	-0.050331	4.815556
239.590788	7999.908831	12.063706	-0.050340	4.815562
239.848117	7999.922650	12.068711	-0.050388	4.815564
239.540971	7999.885640	12.073715	-0.050331	4.815555
239.373665	7999.895752	12.078720	-0.050300	4.815559
239.326470	7999.877921	12.083725	-0.050292	4.815554
239.495284	7999.934078	12.088730	-0.050323	4.815569
239.490892	7999.888113	12.093735	-0.050323	4.815556
239.415734	7999.880505	12.098739	-0.050309	4.815554
239.507653	7999.907648	12.103744	-0.050326	4.815562
239.430122	7999.874375	12.108749	-0.050312	4.815552
239.377872	7999.893833	12.113754	-0.050303	4.815558
239.487324	7999.881754	12.118759	-0.050323	4.815554
239.374241	7999.878868	12.123763	-0.050302	4.815554
239.457731	7999.903739	12.128768	-0.050318	4.815561
239.444069	7999.871504	12.133773	-0.050316	4.815551
239.654247	7999.876013	12.138778	-0.050355	4.815552
239.722566	7999.901705	12.143783	-0.050368	4.815559
239.328728	7999.947639	12.148787	-0.050295	4.815574
239.570811	7999.908888	12.153792	-0.050341	4.815562
239.619051	7999.900084	12.158797	-0.050350	4.815559
239.549616	7999.889366	12.163802	-0.050337	4.815556
239.737022	7999.910589	12.168807	-0.050372	4.815561
239.615178	7999.873390	12.173811	-0.050350	4.815551
239.542670	7999.879706	12.178816	-0.050336	4.815553
239.547686	7999.862725	12.183821	-0.050338	4.815548
239.820306	7999.893876	12.188826	-0.050389	4.815556
239.702373	7999.854606	12.193831	-0.050367	4.815545
239.566334	7999.831058	12.198835	-0.050342	4.815539
239.645397	7999.885755	12.203840	-0.050357	4.815554
239.665578	7999.974731	12.208845	-0.050361	4.815580
239.257848	7999.888034	12.213850	-0.050285	4.815557
239.502774	7999.912328	12.218855	-0.050331	4.815563
239.666775	7999.869103	12.223859	-0.050362	4.815549
239.643989	7999.891177	12.228864	-0.050358	4.815556
239.762142	7999.878172	12.233869	-0.050380	4.815552
239.727713	7999.895785	12.238874	-0.050374	4.815557
239.802798	7999.911978	12.243879	-0.050388	4.815561
239.457124	7999.887154	12.248883	-0.050324	4.815556
239.625493	7999.898457	12.253888	-0.050356	4.815558
239.758222	7999.867537	12.258893	-0.050380	4.815548
239.591866	7999.875529	12.263898	-0.050350	4.815552
239.677389	7999.903636	12.268903	-0.050366	4.815559
239.609649	7999.947402	12.273907	-0.050354	4.815572
239.714651	7999.941658	12.278912	-0.050373	4.815570
239.670633	7999.884370	12.283917	-0.050365	4.815554
239.862317	7999.903527	12.288922	-0.050401	4.815558
239.692589	7999.916803	12.293927	-0.050370	4.815563
239.580015	7999.880824	12.298931	-0.050349	4.815553
239.828942	7999.929742	12.303936	-0.050396	4.815566
239.763601	7999.872108	12.308941	-0.050384	4.815550
239.648695	7999.873462	12.313946	-0.050363	4.815551
239.663707	7999.912168	12.318951	-0.050366	4.815562
239.812600	7999.888985	12.323955	-0.050394	4.815554
239.921614	7999.927086	12.328960	-0.050414	4.815565
239.968305	7999.889426	12.333965	-0.050423	4.815554
239.687458	7999.898758	12.338970	-0.050371	4.815558
239.851372	7999.902515	12.343975	-0.050402	4.815558
239.680061	7999.844224	12.348979	-0.050370	4.815542
239.626613	7999.869002	12.353984	-0.050361	4.815549
239.573675	7999.957856	12.358989	-0.050351	4.815576
239.678168	7999.902985	12.363994	-0.050371	4.815559
239.662424	7999.896343	12.368999	-0.050368	4.815557
239.710370	7999.889670	12.374003	-0.050377	4.815555
239.754864	7999.835958	12.379008	-0.050386	4.815539
239.646729	7999.961286	12.384013	-0.050366	4.815576
239.677750	7999.842220	12.389018	-0.050372	4.815541
239.573208	7999.899268	12.394023	-0.050353	4.815558
239.594724	7999.838776	12.399027	-0.050357	4.815541
239.742887	7999.911682	12.404032	-0.050385	4.815561
239.849210	7999.895281	12.409037	-0.050405	4.815556
239.723508	7999.860155	12.414042	-0.050382	4.815546
239.653720	7999.882532	12.419047	-0.050369	4.815553
239.773086	7999.919733	12.424051	-0.050391	4.815563
239.807431	7999.861585	12.429056	-0.050398	4.815546
239.609874	7999.846646	12.434061	-0.050361	4.815543
239.564728	7999.939897	12.439066	-0.050353	4.815570
239.962860	7999.859907	12.444071	-0.050428	4.815545
239.758406	7999.854465	12.449075	-0.050390	4.815544
239.854352	7999.898759	12.454080	-0.050408	4.815557
239.694754	7999.884438	12.459085	-0.050378	4.815553
239.789004	7999.896671	12.464090	-0.050396	4.815557
239.847073	7999.894433	12.469095	-0.050407	4.815556
239.929643	7999.868036	12.474099	-0.050423	4.815547
240.027766	7999.903823	12.479104	-0.050441	4.815557
239.599827	7999.887270	12.484109	-0.050362	4.815555
239.766118	7999.863303	12.489114	-0.050393	4.815547
239.905543	7999.880542	12.494119	-0.050419	4.815551
239.675005	7999.939811	12.499123	-0.050377	4.815570
239.767383	7999.895421	12.504128	-0.050394	4.815556
239.839882	7999.879537	12.509133	-0.050408	4.815551
239.858722	7999.812594	12.514138	-0.050412	4.815532
239.835820	7999.875242	12.519143	-0.050408	4.815550
239.936496	7999.855546	12.524147	-0.050427	4.815544
239.795764	7999.937633	12.529152	-0.050401	4.815568
239.802352	7999.845931	12.534157	-0.050402	4.815542
239.740678	7999.863101	12.539162	-0.050391	4.815547
239.986548	7999.887412	12.544167	-0.050437	4.815553
239.859625	7999.834113	12.549171	-0.050413	4.815538
239.862176	7999.915328	12.554176	-0.050414	4.815562
239.929937	7999.905774	12.559181	-0.050427	4.815558
239.824930	7999.893409	12.564186	-0.050408	4.815555
239.658843	7999.891795	12.569191	-0.050377	4.815556
239.803570	7999.876019	12.574195	-0.050404	4.815550
239.839069	7999.989804	12.579200	-0.050411	4.815583
239.709223	7999.903356	12.584205	-0.050387	4.815559
239.806953	7999.886816	12.589210	-0.050406	4.815553
239.878105	7999.889063	12.594215	-0.050419	4.815554
239.765389	7999.863758	12.599219	-0.050398	4.815547
239.724269	7999.862043	12.604224	-0.050391	4.815547
239.744037	7999.874131	12.609229	-0.050395	4.815550
239.803352	7999.875118	12.614234	-0.050406	4.815550
239.739856	7999.904004	12.619239	-0.050395	4.815559
239.795948	7999.867565	12.624243	-0.050405	4.815548
239.850001	7999.972042	12.629248	-0.050416	4.815578
240.066208	7999.885887	12.634253	-0.050456	4.815552
239.973349	7999.801109	12.639258	-0.050439	4.815528
240.104447	7999.891891	12.644263	-0.050464	4.815553
239.965616	7999.865093	12.649267	-0.050438	4.815546
239.748337	7999.863714	12.654272	-0.050398	4.815547
239.725577	7999.878314	12.659277	-0.050394	4.815551
239.704288	7999.869447	12.664282	-0.050390	4.815549
239.783572	8000.003164	12.669287	-0.050405	4.815587
239.594971	7999.892269	12.674291	-0.050370	4.815556
239.743328	7999.909654	12.679296	-0.050398	4.815560
239.681763	7999.903334	12.684301	-0.050387	4.815559
239.779988	7999.910293	12.689306	-0.050405	4.815560
239.863916	7999.914883	12.694311	-0.050421	4.815561
239.723641	7999.866707	12.699315	-0.050395	4.815548
239.751175	7999.905617	12.704320	-0.050401	4.815559
239.773395	7999.905999	12.709325	-0.050405	4.815559
239.765986	7999.876002	12.714330	-0.050404	4.815550
239.819036	7999.915327	12.719335	-0.050414	4.815562
239.617097	7999.857605	12.724339	-0.050377	4.815546
240.023175	7999.910149	12.729344	-0.050453	4.815559
240.070967	7999.902406	12.734349	-0.050462	4.815557
239.856753	7999.886128	12.739354	-0.050422	4.815553
239.933417	7999.907684	12.744359	-0.050437	4.815559
239.694859	7999.855773	12.749363	-0.050393	4.815545
239.787559	7999.869048	12.754368	-0.050410	4.815548
239.804372	7999.909919	12.759373	-0.050413	4.815560
239.798187	7999.956823	12.764378	-0.050413	4.815574
239.969609	7999.896634	12.769383	-0.050445	4.815555
239.959359	7999.884743	12.774387	-0.050443	4.815552
239.919268	7999.888383	12.779392	-0.050436	4.815553
239.856371	7999.880973	12.784397	-0.050424	4.815551
239.829561	7999.877355	12.789402	-0.050420	4.815550
239.959705	7999.933952	12.794407	-0.050444	4.815566
239.971618	7999.899997	12.799411	-0.050446	4.815556
240.070748	7999.932598	12.804416	-0.050465	4.815565
240.106942	7999.915056	12.809421	-0.050472	4.815560
240.057469	7999.912136	12.814426	-0.050463	4.815559
240.124197	7999.935668	12.819431	-0.050476	4.815566
239.847444	7999.883134	12.824435	-0.050425	4.815552
240.149109	7999.909420	12.829440	-0.050481	4.815558
240.165697	7999.909712	12.834445	-0.050484	4.815558
239.786229	7999.884337	12.839450	-0.050414	4.815552
239.762080	7999.891440	12.844455	-0.050410	4.815555
239.782100	7999.891787	12.849459	-0.050414	4.815555
239.788052	7999.936752	12.854464	-0.050415	4.815568
239.785560	7999.908970	12.859469	-0.050415	4.815560
239.696747	7999.903275	12.864474	-0.050398	4.815558
239.840602	7999.919518	12.869479	-0.050426	4.815562
239.768648	7999.887403	12.874483	-0.050412	4.815553
239.804816	7999.907233	12.879488	-0.050419	4.815559
239.594610	7999.898494	12.884493	-0.050380	4.815557
239.699335	7999.904491	12.889498	-0.050400	4.815559
239.994908	7999.934950	12.894503	-0.050455	4.815566
239.843749	7999.897273	12.899507	-0.050428	4.815556
239.673961	7999.890260	12.904512	-0.050396	4.815555
239.732958	7999.899784	12.909517	-0.050407	4.815557
239.786041	7999.892127	12.914522	-0.050418	4.815555
239.842984	7999.942193	12.919527	-0.050428	4.815569
239.671373	7999.894574	12.924531	-0.050397	4.815556
239.687650	7999.931165	12.929536	-0.050400	4.815567
239.755613	7999.916276	12.934541	-0.050413	4.815562
239.839747	7999.884565	12.939546	-0.050429	4.815552
239.917519	7999.896529	12.944551	-0.050443	4.815555
239.937756	7999.976965	12.949555	-0.050448	4.815579
239.850772	7999.927519	12.954560	-0.050432	4.815565
239.839947	7999.893195	12.959565	-0.050430	4.815555
239.781046	7999.881580	12.964570	-0.050419	4.815552
239.998062	7999.916099	12.969575	-0.050460	4.815561
239.803518	7999.841412	12.974579	-0.050424	4.815540
239.962392	7999.885663	12.979584	-0.050454	4.815552
239.885049	7999.888696	12.984589	-0.050439	4.815553
239.899091	7999.882539	12.989594	-0.050442	4.815551
239.938942	7999.928057	12.994599	-0.050450	4.815564
239.785699	7999.902092	12.999603	-0.050422	4.815557
239.980523	7999.937318	13.004608	-0.050458	4.815567
239.853353	7999.894693	13.009613	-0.050435	4.815555
239.931870	7999.910942	13.014618	-0.050450	4.815559
240.047830	7999.918189	13.019623	-0.050471	4.815561
239.842320	7999.892442	13.024627	-0.050433	4.815554
239.835099	7999.921176	13.029632	-0.050432	4.815563
240.141435	7999.922980	13.034637	-0.050490	4.815562
239.951153	7999.895345	13.039642	-0.050454	4.815555
239.848354	7999.918252	13.044647	-0.050435	4.815562
239.860612	7999.898185	13.049651	-0.050438	4.815556
239.909852	7999.903279	13.054656	-0.050447	4.815557
239.825320	7999.901924	13.059661	-0.050432	4.815557
239.942020	7999.854726	13.064666	-0.050454	4.815543
239.826333	7999.907322	13.069671	-0.050433	4.815559
239.850757	7999.884249	13.074675	-0.050437	4.815552
240.035367	7999.933191	13.079680	-0.050472	4.815565
240.130283	7999.904858	13.084685	-0.050490	4.815557
239.886018	7999.986328	13.089690	-0.050445	4.815582
240.056362	7999.912240	13.094695	-0.050477	4.815559
239.954147	7999.888174	13.099699	-0.050458	4.815552
239.963788	7999.919318	13.104704	-0.050460	4.815562
239.971140	7999.916256	13.109709	-0.050461	4.815561
239.994520	7999.914522	13.114714	-0.050466	4.815560
240.077969	7999.921240	13.119719	-0.050482	4.815562
239.979639	7999.895102	13.124723	-0.050464	4.815554
239.877592	7999.912682	13.129728	-0.050445	4.815560
239.959556	7999.924716	13.134733	-0.050461	4.815563
239.863426	7999.943460	13.139738	-0.050443	4.815569
239.849756	7999.935785	13.144743	-0.050441	4.815567
239.860195	7999.911416	13.149747	-0.050443	4.815560
239.988317	7999.931675	13.154752	-0.050467	4.815565
239.902277	7999.889720	13.159757	-0.050451	4.815553
239.918310	7999.906019	13.164762	-0.050454	4.815558
240.023069	7999.917356	13.169767	-0.050474	4.815561
239.819259	7999.907653	13.174771	-0.050436	4.815559
240.127810	7999.927645	13.179776	-0.050494	4.815563
240.221031	7999.912099	13.184781	-0.050512	4.815558
239.930378	7999.923407	13.189786	-0.050458	4.815563
239.930698	7999.938382	13.194791	-0.050458	4.815567
240.004222	7999.906498	13.199795	-0.050472	4.815557
240.018744	7999.920637	13.204800	-0.050475	4.815562
239.953156	7999.911049	13.209805	-0.050463	4.815559
239.804344	7999.891563	13.214810	-0.050436	4.815554
239.918163	7999.926539	13.219815	-0.050457	4.815564
239.799975	7999.877653	13.224819	-0.050435	4.815550
239.900838	7999.909214	13.229824	-0.050454	4.815559
240.088446	7999.902679	13.234829	-0.050489	4.815556
239.969719	7999.910378	13.239834	-0.050468	4.815559
240.033502	7999.914641	13.244839	-0.050480	4.815560
239.801935	7999.901283	13.249843	-0.050437	4.815557
240.042977	7999.882803	13.254848	-0.050482	4.815550
240.049332	7999.894674	13.259853	-0.050483	4.815554
239.784626	7999.865828	13.264858	-0.050434	4.815547
240.134546	7999.922798	13.269863	-0.050500	4.815562
239.837673	7999.892360	13.274867	-0.050445	4.815554
239.773376	7999.947928	13.279872	-0.050433	4.815571
239.864030	7999.917391	13.284877	-0.050450	4.815561
239.716655	7999.891522	13.289882	-0.050423	4.815554
239.910446	7999.937409	13.294887	-0.050459	4.815567
239.979943	7999.895850	13.299891	-0.050472	4.815554
239.857235	7999.933383	13.304896	-0.050450	4.815566
239.916998	7999.918359	13.309901	-0.050461	4.815561
239.809518	7999.916631	13.314906	-0.050441	4.815561
240.117639	7999.947295	13.319911	-0.050499	4.815569
239.981132	7999.892772	13.324915	-0.050474	4.815553
239.893804	7999.926609	13.329920	-0.050458	4.815564
239.973889	7999.921527	13.334925	-0.050473	4.815562
240.169465	7999.936478	13.339930	-0.050510	4.815565
240.091212	7999.959785	13.344935	-0.050495	4.815572
239.779085	7999.908810	13.349939	-0.050437	4.815559
239.866180	7999.951893	13.354944	-0.050454	4.815571
240.010428	7999.915821	13.359949	-0.050481	4.815560
239.961505	7999.920385	13.364954	-0.050472	4.815562
239.998916	7999.929558	13.369959	-0.050479	4.815564
239.778167	7999.908901	13.374963	-0.050438	4.815559
240.077726	7999.923409	13.379968	-0.050494	4.815562
240.003934	7999.914754	13.384973	-0.050481	4.815560
239.912751	7999.897274	13.389978	-0.050464	4.815555
240.153064	7999.922563	13.394983	-0.050509	4.815561
239.974597	7999.887645	13.399987	-0.050476	4.815552
240.085718	7999.915102	13.404992	-0.050497	4.815559
239.938354	7999.923403	13.409997	-0.050470	4.815562
239.917761	7999.910276	13.415002	-0.050466	4.815559
240.141652	7999.926755	13.420007	-0.050508	4.815562
240.086778	7999.924815	13.425011	-0.050498	4.815562
239.908147	7999.951827	13.430016	-0.050465	4.815571
239.814985	7999.931111	13.435021	-0.050448	4.815565
239.978405	7999.918843	13.440026	-0.050479	4.815561
240.042480	7999.944467	13.445031	-0.050491	4.815568
239.909267	7999.907083	13.450035	-0.050466	4.815558
240.046805	7999.916817	13.455040	-0.050492	4.815560
239.856303	7999.907331	13.460045	-0.050457	4.815558
239.864702	7999.896811	13.465050	-0.050459	4.815555
240.098091	7999.939072	13.470055	-0.050503	4.815566
240.107329	7999.980888	13.475059	-0.050505	4.815578
240.082765	7999.919644	13.480064	-0.050500	4.815561
239.911180	7999.924347	13.485069	-0.050469	4.815563
239.884075	7999.848114	13.490074	-0.050464	4.815541
240.158720	7999.899588	13.495079	-0.050515	4.815554
240.126713	7999.869190	13.500083	-0.050509	4.815546
240.100378	7999.849562	13.505088	-0.050505	4.815540
240.180692	7999.898942	13.510093	-0.050520	4.815554
239.817130	7999.880232	13.515098	-0.050452	4.815550
239.916653	7999.890415	13.520103	-0.050471	4.815553
239.956667	7999.866528	13.525107	-0.050479	4.815546
239.973850	7999.913813	13.530112	-0.050482	4.815559
239.868211	7999.902504	13.535117	-0.050463	4.815557
240.205077	7999.909076	13.540122	-0.050526	4.815557
240.240220	7999.952382	13.545127	-0.050533	4.815569
240.111504	7999.894782	13.550131	-0.050509	4.815553
240.086046	7999.924287	13.555136	-0.050505	4.815562
240.236934	7999.929968	13.560141	-0.050533	4.815563
240.229248	7999.896762	13.565146	-0.050532	4.815553
240.291078	7999.942638	13.570151	-0.050543	4.815566
240.127491	7999.907962	13.575155	-0.050513	4.815557
240.159561	7999.923455	13.580160	-0.050519	4.815561
240.058176	7999.931436	13.585165	-0.050501	4.815564
239.971215	7999.898008	13.590170	-0.050485	4.815555
240.128461	7999.943300	13.595175	-0.050514	4.815567
239.902178	7999.917215	13.600179	-0.050472	4.815561
240.117498	7999.934622	13.605184	-0.050513	4.815565
240.237474	7999.917376	13.610189	-0.050535	4.815559
239.878799	7999.894474	13.615194	-0.050469	4.815554
240.106799	7999.949461	13.620199	-0.050512	4.815569
240.337197	7999.925470	13.625203	-0.050555	4.815561
240.337150	7999.932965	13.630208	-0.050555	4.815563
240.201085	7999.939314	13.635213	-0.050530	4.815566
240.202864	7999.941499	13.640218	-0.050530	4.815566
240.268193	7999.960737	13.645223	-0.050543	4.815572
240.184360	7999.916681	13.650227	-0.050527	4.815559
240.198863	7999.943634	13.655232	-0.050530	4.815567
240.203946	7999.922381	13.660237	-0.050532	4.815561
240.096365	7999.934533	13.665242	-0.050512	4.815565
240.122574	7999.940320	13.670247	-0.050517	4.815566
240.136863	7999.863692	13.675251	-0.050520	4.815544
240.096323	7999.883341	13.680256	-0.050512	4.815550
240.187793	7999.881648	13.685261	-0.050530	4.815549
240.156852	7999.898251	13.690266	-0.050524	4.815554
240.499223	7999.926269	13.695271	-0.050588	4.815560
240.369513	7999.913501	13.700275	-0.050564	4.815557
240.297102	7999.936903	13.705280	-0.050551	4.815564
240.429012	7999.908105	13.710285	-0.050576	4.815555
240.404736	7999.884239	13.715290	-0.050572	4.815548
240.219660	7999.926096	13.720295	-0.050537	4.815562
240.069441	7999.904451	13.725299	-0.050510	4.815556
240.265608	7999.922615	13.730304	-0.050546	4.815560
240.286702	7999.893081	13.735309	-0.050551	4.815552
240.066750	7999.899132	13.740314	-0.050510	4.815554
240.314439	7999.942694	13.745319	-0.050556	4.815566
240.155579	7999.912366	13.750323	-0.050527	4.815558
240.031037	7999.927445	13.755328	-0.050504	4.815563
240.139968	7999.929239	13.760333	-0.050525	4.815563
240.259561	7999.901309	13.765338	-0.050547	4.815554
240.222693	7999.934900	13.770343	-0.050540	4.815564
240.056412	7999.981333	13.775347	-0.050510	4.815578
240.184175	7999.932180	13.780352	-0.050534	4.815563
240.224766	7999.930726	13.785357	-0.050542	4.815563
240.159922	7999.910471	13.790362	-0.050530	4.815557
240.410811	7999.945543	13.795367	-0.050577	4.815566
240.137538	7999.909082	13.800371	-0.050526	4.815557
240.307107	7999.913999	13.805376	-0.050558	4.815557
240.499790	7999.924632	13.810381	-0.050594	4.815560
240.397377	7999.912307	13.815386	-0.050575	4.815557
240.393834	7999.937899	13.820391	-0.050575	4.815564
240.237964	7999.899077	13.825395	-0.050546	4.815553
240.406340	7999.930670	13.830400	-0.050578	4.815562
240.480324	7999.916946	13.835405	-0.050592	4.815557
240.146166	7999.917934	13.840410	-0.050530	4.815559
240.222052	7999.952293	13.845415	-0.050544	4.815569
240.439768	7999.914214	13.850419	-0.050585	4.815557
240.371287	7999.930205	13.855424	-0.050572	4.815562
240.319445	7999.937925	13.860429	-0.050563	4.815564
240.435816	7999.909942	13.865434	-0.050585	4.815556
240.318953	7999.931553	13.870439	-0.050563	4.815562
240.142417	7999.913751	13.875443	-0.050531	4.815558
240.320348	7999.940160	13.880448	-0.050564	4.815565
240.563332	7999.950545	13.885453	-0.050609	4.815567
240.408880	7999.925627	13.890458	-0.050581	4.815560
240.407905	7999.936311	13.895463	-0.050581	4.815563
240.338858	7999.881817	13.900467	-0.050568	4.815548
240.386347	7999.938138	13.905472	-0.050577	4.815564
240.488550	7999.923806	13.910477	-0.050597	4.815559
240.449387	7999.916782	13.915482	-0.050590	4.815557
240.213553	7999.939660	13.920487	-0.050546	4.815565
240.042436	7999.908064	13.925491	-0.050514	4.815557
240.242177	7999.930558	13.930496	-0.050552	4.815562
240.242365	7999.923107	13.935501	-0.050552	4.815560
239.840406	7999.879213	13.940506	-0.050477	4.815549
240.059866	7999.941535	13.945511	-0.050519	4.815567
240.013787	7999.911976	13.950515	-0.050510	4.815558
240.183102	7999.922228	13.955520	-0.050542	4.815560
240.014751	7999.916305	13.960525	-0.050511	4.815559
240.073298	7999.941839	13.965530	-0.050522	4.815567
240.063278	7999.947036	13.970535	-0.050520	4.815568
239.810007	7999.906629	13.975539	-0.050474	4.815557
240.145950	7999.915322	13.980544	-0.050536	4.815558
240.244282	7999.921215	13.985549	-0.050555	4.815560
240.045498	7999.920136	13.990554	-0.050518	4.815560
240.146230	7999.914323	13.995559	-0.050537	4.815558
240.204377	7999.889663	14.000563	-0.050548	4.815551
240.312837	7999.936298	14.005568	-0.050569	4.815564
240.215906	7999.906978	14.010573	-0.050551	4.815556
240.081525	7999.903744	14.015578	-0.050526	4.815555
240.323402	7999.916245	14.020583	-0.050571	4.815558
240.287476	7999.882580	14.025587	-0.050565	4.815548
240.296100	7999.927589	14.030592	-0.050567	4.815561
240.322967	7999.924845	14.035597	-0.050572	4.815560
240.218829	7999.889000	14.040602	-0.050553	4.815550
240.425459	7999.904132	14.045607	-0.050592	4.815554
240.629799	7999.877581	14.050611	-0.050630	4.815545
240.508457	7999.899118	14.055616	-0.050607	4.815552
240.205125	7999.917693	14.060621	-0.050551	4.815559
240.358423	7999.915939	14.065626	-0.050580	4.815557
240.446468	7999.934479	14.070631	-0.050597	4.815562
240.276541	7999.884750	14.075635	-0.050565	4.815549
240.264919	7999.920887	14.080640	-0.050563	4.815559
240.478450	7999.917978	14.085645	-0.050603	4.815557
240.553513	7999.940578	14.090650	-0.050618	4.815564
240.427597	7999.958837	14.095655	-0.050594	4.815570
240.325109	7999.930495	14.100659	-0.050576	4.815562
240.400905	7999.938157	14.105664	-0.050590	4.815564
240.510731	7999.916474	14.110669	-0.050611	4.815557
240.430195	7999.895964	14.115674	-0.050596	4.815551
240.505524	7999.939924	14.120679	-0.050610	4.815564
240.406153	7999.904157	14.125683	-0.050592	4.815554
240.563193	7999.933431	14.130688	-0.050621	4.815562
240.664924	7999.934041	14.135693	-0.050640	4.815561
240.550468	7999.934334	14.140698	-0.050619	4.815562
240.456441	7999.936028	14.145703	-0.050602	4.815563
240.475177	7999.913930	14.150707	-0.050606	4.815556
240.498598	7999.915400	14.155712	-0.050610	4.815557
240.526633	7999.923352	14.160717	-0.050616	4.815559
240.407293	7999.919295	14.165722	-0.050594	4.815558
240.386468	7999.920045	14.170727	-0.050590	4.815558
240.335164	7999.901078	14.175731	-0.050581	4.815553
240.351003	7999.913103	14.180736	-0.050584	4.815557
240.286115	7999.920611	14.185741	-0.050572	4.815559
240.335295	7999.920365	14.190746	-0.050582	4.815559
240.514644	7999.945730	14.195751	-0.050615	4.815565
240.478984	7999.940900	14.200755	-0.050609	4.815564
240.615040	7999.917508	14.205760	-0.050635	4.815557
240.518813	7999.926641	14.210765	-0.050617	4.815560
240.265704	7999.862744	14.215770	-0.050570	4.815542
240.616076	7999.910114	14.220775	-0.050636	4.815554
240.610954	7999.922866	14.225779	-0.050635	4.815558
240.525618	7999.934312	14.230784	-0.050619	4.815562
240.632232	7999.924323	14.235789	-0.050639	4.815558
240.646148	7999.924571	14.240794	-0.050642	4.815558
240.660067	7999.931225	14.245799	-0.050645	4.815560
240.658286	7999.663196	14.250803	-0.050645	4.815482

240.654355	7996.393857	14.255808	-0.050642	4.814526
240.519512	7990.811282	14.260813	-0.050614	4.812894
240.522294	7983.954779	14.265818	-0.050610	4.810888
240.477302	7976.683459	14.270823	-0.050597	4.808759
240.514148	7969.076654	14.275827	-0.050599	4.806531
240.444402	7961.212865	14.280832	-0.050581	4.804228
240.341531	7953.434368	14.285837	-0.050557	4.801948
240.247395	7945.368131	14.290842	-0.050535	4.799583
240.300490	7937.422973	14.295847	-0.050540	4.797251
240.182068	7929.364338	14.300851	-0.050513	4.794886
240.124729	7921.406253	14.305856	-0.050497	4.792549
240.180958	7913.381464	14.310861	-0.050502	4.790191
240.150682	7905.393376	14.315866	-0.050492	4.787842
240.224789	7897.425523	14.320871	-0.050501	4.785498
240.087878	7889.432167	14.325875	-0.050470	4.783146
239.989809	7881.366998	14.330880	-0.050447	4.780772
240.040460	7873.468900	14.335885	-0.050452	4.778445
239.981759	7865.405885	14.340890	-0.050436	4.776069
239.917628	7857.427290	14.345895	-0.050419	4.773717
239.826625	7849.379321	14.350899	-0.050397	4.771343
239.754705	7841.335638	14.355904	-0.050378	4.768969
239.833576	7833.436299	14.360909	-0.050388	4.766636
239.831168	7825.345449	14.365914	-0.050383	4.764245
239.921956	7817.417098	14.370919	-0.050395	4.761901
239.712521	7809.343483	14.375923	-0.050351	4.759514
239.448223	7801.368311	14.380928	-0.050296	4.757155
239.576017	7793.398464	14.385933	-0.050315	4.754795
239.468778	7785.310852	14.390938	-0.050290	4.752400
239.530724	7777.336639	14.395943	-0.050297	4.750037
239.232466	7769.303574	14.400947	-0.050236	4.747656
239.414281	7761.303904	14.405952	-0.050265	4.745282
239.443216	7753.382318	14.410957	-0.050266	4.742931
239.337608	7745.293014	14.415962	-0.050241	4.740529
239.488424	7737.384800	14.420967	-0.050264	4.738179
239.323511	7729.323027	14.425971	-0.050228	4.735783
239.201357	7721.327736	14.430976	-0.050201	4.733406
239.060776	7713.282846	14.435981	-0.050170	4.731013
238.862272	7705.289788	14.440986	-0.050128	4.728634
238.896703	7697.317594	14.445991	-0.050129	4.726259
239.012509	7689.262132	14.450995	-0.050146	4.723858
239.001164	7681.299671	14.456000	-0.050139	4.721484
238.880440	7673.329847	14.461005	-0.050111	4.719107
238.720658	7665.374232	14.466010	-0.050076	4.716733
238.825075	7657.339089	14.471015	-0.050091	4.714334
239.009295	7649.303403	14.476019	-0.050120	4.711933
238.955554	7641.267854	14.481024	-0.050105	4.709531
238.858946	7633.301867	14.486029	-0.050082	4.707149
238.645745	7625.271312	14.491034	-0.050038	4.704746
238.728277	7617.351286	14.496039	-0.050048	4.702375
238.698758	7609.304206	14.501043	-0.050038	4.699965
238.645294	7601.369434	14.506048	-0.050023	4.697587
238.686912	7593.305031	14.511053	-0.050025	4.695169
238.572523	7585.254204	14.516058	-0.049999	4.692754
238.651567	7577.268020	14.521063	-0.050009	4.690357
238.389615	7569.266230	14.526067	-0.049955	4.687955
238.598662	7561.263006	14.531072	-0.049989	4.685550
238.539871	7553.345421	14.536077	-0.049973	4.683170
238.397017	7545.291344	14.541082	-0.049942	4.680748
238.437258	7537.335783	14.546087	-0.049944	4.678354
238.475438	7529.317927	14.551091	-0.049946	4.675940
238.264564	7521.243971	14.556096	-0.049902	4.673509
238.147912	7513.173696	14.561101	-0.049875	4.671076
238.068707	7505.167875	14.566106	-0.049856	4.668663
238.261509	7497.292535	14.571111	-0.049887	4.666286
238.460682	7489.206084	14.576115	-0.049919	4.663845
238.305765	7481.259934	14.581120	-0.049885	4.661446
238.136703	7473.268311	14.586125	-0.049848	4.659031
238.062841	7465.218244	14.591130	-0.049830	4.656598
238.019235	7457.213793	14.596135	-0.049817	4.654176
237.930850	7449.241245	14.601139	-0.049795	4.651764
237.684411	7441.178637	14.606144	-0.049744	4.649323
237.866500	7433.280125	14.611149	-0.049773	4.646930
237.859436	7425.164810	14.616154	-0.049767	4.644470
237.737289	7417.257332	14.621159	-0.049739	4.642072
237.756908	7409.190722	14.626163	-0.049738	4.639624
237.659599	7401.252559	14.631168	-0.049715	4.637214
237.675307	7393.270454	14.636173	-0.049713	4.634790
237.684701	7385.161059	14.641178	-0.049709	4.632325
237.768979	7377.168988	14.646183	-0.049720	4.629895
237.532238	7369.202306	14.651187	-0.049671	4.627471
237.544900	7361.162173	14.656192	-0.049669	4.625024
237.737581	7353.216598	14.661197	-0.049699	4.622604
237.383706	7345.175522	14.666202	-0.049629	4.620154
237.345044	7337.233118	14.671207	-0.049616	4.617733
237.433476	7329.184401	14.676211	-0.049628	4.615278
237.256904	7321.190091	14.681216	-0.049590	4.612838
237.193549	7313.146897	14.686221	-0.049573	4.610382
236.938186	7305.171463	14.691226	-0.049521	4.607945
237.028967	7297.132714	14.696231	-0.049533	4.605488
236.944323	7289.184111	14.701235	-0.049512	4.603056
236.944523	7281.148878	14.706240	-0.049507	4.600598
236.940383	7273.186254	14.711245	-0.049501	4.598160
236.785519	7265.157788	14.716250	-0.049467	4.595700
236.943065	7257.122974	14.721255	-0.049492	4.593237
236.968815	7249.116075	14.726259	-0.049492	4.590782
236.997846	7241.167363	14.731264	-0.049492	4.588343
236.767551	7233.155347	14.736269	-0.049444	4.585883
236.643281	7225.121046	14.741274	-0.049416	4.583415
236.495185	7217.134862	14.746279	-0.049384	4.580961
236.458091	7209.126316	14.751283	-0.049372	4.578498
236.286792	7201.160046	14.756288	-0.049335	4.576047
236.324355	7193.116327	14.761293	-0.049337	4.573571
236.211157	7185.062275	14.766298	-0.049311	4.571090
236.288076	7177.099059	14.771303	-0.049320	4.568636
236.167787	7169.139842	14.776307	-0.049293	4.566182
236.160044	7161.113685	14.781312	-0.049286	4.563706
236.124053	7153.171897	14.786317	-0.049275	4.561255
236.157442	7145.138084	14.791322	-0.049276	4.558774
236.207668	7137.196440	14.796327	-0.049280	4.556320
236.341561	7129.123383	14.801331	-0.049300	4.553824
236.326694	7121.096817	14.806336	-0.049293	4.551341
236.233092	7113.117408	14.811341	-0.049270	4.548871
236.103702	7105.116364	14.816346	-0.049241	4.546393
236.141526	7097.102692	14.821351	-0.049243	4.543910
236.051408	7089.131382	14.826355	-0.049221	4.541439
235.861806	7081.072474	14.831360	-0.049181	4.538939
235.959422	7073.169182	14.836365	-0.049194	4.536486
235.863356	7065.100493	14.841370	-0.049171	4.533981
235.995883	7057.118193	14.846375	-0.049191	4.531501
235.773706	7049.092406	14.851379	-0.049145	4.529005
235.782034	7041.152828	14.856384	-0.049141	4.526536
235.749200	7033.124610	14.861389	-0.049130	4.524037
235.374714	7025.126401	14.866394	-0.049056	4.521546
235.428271	7017.131543	14.871399	-0.049061	4.519055
235.431482	7009.164497	14.876403	-0.049056	4.516572
235.514757	7001.077123	14.881408	-0.049067	4.514049
235.402593	6993.041831	14.886413	-0.049041	4.511542
235.235899	6984.987522	14.891418	-0.049005	4.509026
235.305342	6977.034678	14.896423	-0.049013	4.506542
235.198704	6969.059772	14.901427	-0.048988	4.504048
235.341932	6961.059174	14.906432	-0.049010	4.501546
235.229036	6953.098209	14.911437	-0.048984	4.499055
235.097309	6945.076092	14.916442	-0.048954	4.496542
235.032182	6937.067852	14.921447	-0.048937	4.494033
234.963444	6929.043243	14.926451	-0.048919	4.491518
234.971511	6921.013454	14.931456	-0.048916	4.488999
235.171430	6913.095652	14.936461	-0.048948	4.486515
234.922285	6905.027716	14.941466	-0.048897	4.483981
235.053293	6897.082678	14.946471	-0.048916	4.481485
235.006270	6889.051574	14.951475	-0.048902	4.478960
234.728978	6881.061251	14.956480	-0.048846	4.476446
234.795496	6873.060844	14.961485	-0.048853	4.473929
234.858865	6864.994583	14.966490	-0.048860	4.471389
234.783331	6857.040465	14.971495	-0.048841	4.468882
234.509984	6849.015912	14.976499	-0.048785	4.466352
234.642333	6841.016975	14.981504	-0.048805	4.463829
234.649076	6833.081375	14.986509	-0.048801	4.461325
234.586615	6824.999857	14.991514	-0.048785	4.458772
234.667136	6817.055574	14.996519	-0.048795	4.456263
234.553878	6808.988843	15.001523	-0.048768	4.453712
234.262293	6800.980366	15.006528	-0.048709	4.451178
234.301926	6793.003844	15.011533	-0.048712	4.448653
234.132665	6785.016845	15.016538	-0.048675	4.446123
234.352657	6777.007611	15.021543	-0.048711	4.443586
234.267811	6769.049322	15.026547	-0.048690	4.441063
234.283888	6761.006650	15.031552	-0.048688	4.438511
234.209121	6753.050498	15.036557	-0.048670	4.435986
233.906944	6744.946847	15.041562	-0.048608	4.433411
233.892224	6736.975533	15.046567	-0.048601	4.430877
234.069220	6728.967733	15.051571	-0.048629	4.428332
233.848508	6720.957558	15.056576	-0.048582	4.425783
233.894491	6712.993229	15.061581	-0.048586	4.423248
233.827805	6704.995957	15.066586	-0.048569	4.420700
233.680258	6697.002603	15.071591	-0.048536	4.418152
233.762192	6688.983955	15.076595	-0.048547	4.415595
233.660266	6680.958130	15.081600	-0.048523	4.413034
233.967986	6672.989183	15.086605	-0.048575	4.410491
233.717177	6664.992632	15.091610	-0.048523	4.407936
233.573989	6656.951233	15.096615	-0.048492	4.405365
233.506580	6648.996302	15.101619	-0.048474	4.402820
233.573628	6640.971593	15.106624	-0.048482	4.400253
233.609552	6633.036879	15.111629	-0.048483	4.397712
233.629000	6625.041750	15.116634	-0.048482	4.395151
233.512317	6616.972809	15.121639	-0.048455	4.392564
233.329071	6608.969191	15.126643	-0.048416	4.389996
233.344992	6600.956139	15.131648	-0.048414	4.387424
233.516726	6592.977089	15.136653	-0.048441	4.384863
233.273009	6585.027590	15.141658	-0.048391	4.382307
233.430945	6576.986226	15.146663	-0.048415	4.379723
233.451632	6569.011255	15.151667	-0.048414	4.377157
233.376181	6560.988442	15.156672	-0.048395	4.374575
233.319006	6553.005917	15.161677	-0.048380	4.372003
233.219495	6544.948536	15.166682	-0.048356	4.369406
233.137822	6537.011801	15.171687	-0.048336	4.366846
232.930068	6528.967083	15.176691	-0.048292	4.364249
232.961241	6521.012488	15.181696	-0.048293	4.361682
233.208690	6513.003239	15.186701	-0.048334	4.359096
232.813504	6505.073239	15.191706	-0.048256	4.356530
232.958984	6496.990524	15.196711	-0.048278	4.353917
232.981676	6488.876524	15.201715	-0.048277	4.351292
232.903056	6480.928536	15.206720	-0.048257	4.348718
232.661160	6472.937612	15.211725	-0.048207	4.346127
232.664654	6464.927182	15.216730	-0.048203	4.343530
232.680839	6456.943410	15.221735	-0.048201	4.340940
232.683924	6448.997375	15.226739	-0.048197	4.338361
232.588080	6440.947680	15.231744	-0.048174	4.335746
232.655897	6432.957929	15.236749	-0.048181	4.333150
232.603094	6424.893994	15.241754	-0.048167	4.330528
232.650235	6416.950760	15.246759	-0.048170	4.327944
232.472243	6408.965493	15.251763	-0.048132	4.325343
232.415087	6400.977608	15.256768	-0.048117	4.322740
232.453486	6392.964635	15.261773	-0.048119	4.320129
232.417885	6384.956273	15.266778	-0.048107	4.317517
232.433780	6376.942988	15.271783	-0.048105	4.314902
232.268695	6368.937803	15.276787	-0.048070	4.312286
232.010398	6360.902476	15.281792	-0.048016	4.309659
232.371894	6352.958734	15.286797	-0.048079	4.307064
232.230524	6344.884675	15.291802	-0.048048	4.304422
232.038832	6336.951280	15.296807	-0.048007	4.301823
231.969041	6328.920719	15.301811	-0.047989	4.299193
232.105800	6320.964357	15.306816	-0.048009	4.296586
231.999892	6312.968292	15.311821	-0.047985	4.293963
231.774152	6304.897381	15.316826	-0.047938	4.291313
231.927485	6296.883886	15.321831	-0.047961	4.288683
231.772507	6288.955196	15.326835	-0.047927	4.286076
231.613772	6280.887191	15.331840	-0.047893	4.283423
231.818501	6272.980068	15.336845	-0.047926	4.280823
231.693799	6264.911675	15.341850	-0.047898	4.278166
231.740533	6256.950042	15.346855	-0.047902	4.275545
231.664948	6248.913136	15.351859	-0.047883	4.272895
231.475117	6240.859650	15.356864	-0.047842	4.270238
231.451909	6232.903322	15.361869	-0.047833	4.267612
231.460622	6224.868820	15.366874	-0.047830	4.264959
231.731388	6216.904072	15.371879	-0.047875	4.262330
231.699527	6208.882466	15.376883	-0.047864	4.259678
231.376850	6200.932299	15.381888	-0.047799	4.257046
231.466961	6192.920224	15.386893	-0.047811	4.254394
231.398858	6184.901470	15.391898	-0.047793	4.251738
231.355445	6176.864474	15.396903	-0.047780	4.249074
231.320285	6168.947128	15.401907	-0.047769	4.246448
231.278098	6160.904165	15.406912	-0.047756	4.243779
231.393791	6152.948275	15.411917	-0.047772	4.241138
231.100308	6144.928222	15.416922	-0.047713	4.238471
231.047688	6136.976814	15.421927	-0.047698	4.235827
231.199989	6128.913751	15.426931	-0.047721	4.233146
231.024635	6120.885935	15.431936	-0.047684	4.230472
231.042319	6112.915692	15.436941	-0.047682	4.227817
231.050559	6104.896424	15.441946	-0.047679	4.225144
231.008613	6096.934261	15.446951	-0.047666	4.222488
230.854646	6088.918765	15.451955	-0.047632	4.219812
230.797213	6080.957852	15.456960	-0.047617	4.217153
230.781644	6072.929733	15.461965	-0.047609	4.214470
230.692837	6064.912711	15.466970	-0.047587	4.211789
230.737639	6056.896730	15.471975	-0.047591	4.209107
230.700879	6048.949897	15.476979	-0.047579	4.206446
230.487848	6040.915780	15.481984	-0.047534	4.203753
230.508070	6033.013669	15.486989	-0.047533	4.201104
230.570242	6024.937503	15.491994	-0.047540	4.198396
230.622671	6016.950526	15.496999	-0.047544	4.195715
230.676193	6008.875678	15.502003	-0.047549	4.193004
230.497361	6000.831141	15.507008	-0.047511	4.190298
230.362611	5992.916670	15.512013	-0.047481	4.187635
230.146091	5984.876400	15.517018	-0.047436	4.184927
229.958691	5976.929454	15.522023	-0.047396	4.182249
230.077538	5968.910925	15.527027	-0.047413	4.179549
229.827979	5960.916199	15.532032	-0.047362	4.176850
230.219655	5952.898020	15.537037	-0.047430	4.174149
230.113824	5944.849753	15.542042	-0.047405	4.171431
230.316490	5936.873081	15.547047	-0.047438	4.168739
230.161640	5928.908045	15.552051	-0.047404	4.166044
230.160723	5920.915314	15.557056	-0.047399	4.163341
230.034944	5912.944965	15.562061	-0.047370	4.160642
229.764551	5904.907423	15.567066	-0.047315	4.157916
229.981397	5896.906287	15.572071	-0.047350	4.155207
229.939439	5888.895370	15.577075	-0.047338	4.152489
229.786263	5880.848553	15.582080	-0.047304	4.149757
229.799442	5872.922562	15.587085	-0.047302	4.147065
229.664512	5864.849909	15.592090	-0.047271	4.144320
229.566854	5856.921766	15.597095	-0.047248	4.141623
229.385163	5848.908285	15.602099	-0.047210	4.138894
229.536895	5840.902843	15.607104	-0.047233	4.136170
229.700825	5832.885691	15.612109	-0.047258	4.133441
229.489351	5824.833414	15.617114	-0.047214	4.130693
229.455109	5816.908182	15.622119	-0.047203	4.127988
229.415297	5808.905177	15.627123	-0.047190	4.125256
229.366891	5800.895027	15.632128	-0.047176	4.122519
229.301746	5792.929189	15.637133	-0.047159	4.119795
229.360007	5784.944888	15.642138	-0.047165	4.117064
229.334358	5776.922516	15.647143	-0.047155	4.114318
229.329441	5768.867380	15.652147	-0.047149	4.111559
229.041329	5760.854800	15.657152	-0.047091	4.108808
229.166456	5752.868362	15.662157	-0.047109	4.106071
228.928150	5744.884756	15.667162	-0.047060	4.103327
228.911774	5736.892601	15.672167	-0.047052	4.100582
229.008014	5728.903271	15.677171	-0.047065	4.097838
228.810442	5720.913441	15.682176	-0.047023	4.095087
229.005624	5712.911910	15.687181	-0.047054	4.092336
228.943470	5704.885008	15.692186	-0.047038	4.089571
228.926391	5696.921560	15.697191	-0.047030	4.086826
228.798654	5688.904512	15.702195	-0.047001	4.084060
228.823461	5680.927577	15.707200	-0.047001	4.081308
229.141326	5672.956941	15.712205	-0.047055	4.078560
228.709904	5664.968404	15.717210	-0.046970	4.075793
228.790690	5656.925963	15.722215	-0.046980	4.073013
228.802594	5648.892686	15.727219	-0.046977	4.070234
228.695721	5640.887772	15.732224	-0.046952	4.067461
228.685217	5632.887120	15.737229	-0.046945	4.064688
228.663108	5624.953622	15.742234	-0.046936	4.061937
228.619460	5616.946351	15.747239	-0.046923	4.059158
228.442865	5608.995959	15.752243	-0.046885	4.056395
228.133977	5600.923651	15.757248	-0.046823	4.053586
228.224932	5592.917488	15.762253	-0.046834	4.050804
228.115672	5584.913575	15.767258	-0.046809	4.048017
227.946439	5576.925833	15.772263	-0.046773	4.045234
228.261552	5568.970533	15.777267	-0.046826	4.042467
228.032285	5560.919399	15.782272	-0.046779	4.039656
228.012095	5552.983964	15.787277	-0.046770	4.036887
228.024707	5544.905974	15.792282	-0.046767	4.034067
227.916572	5536.842439	15.797287	-0.046742	4.031249
227.691765	5528.871797	15.802291	-0.046695	4.028458
227.651090	5520.868399	15.807296	-0.046683	4.025658
227.691625	5512.918731	15.812301	-0.046685	4.022875
227.588421	5504.890923	15.817306	-0.046661	4.020061
227.398231	5496.925157	15.822311	-0.046621	4.017265
227.678024	5488.904087	15.827315	-0.046668	4.014455
227.780919	5480.869758	15.832320	-0.046682	4.011636
227.575493	5472.908173	15.837325	-0.046639	4.008836
227.269379	5464.926601	15.842330	-0.046577	4.006025
227.355316	5456.917056	15.847335	-0.046588	4.003208
227.452009	5448.933017	15.852339	-0.046601	4.000398
227.441417	5440.927561	15.857344	-0.046594	3.997578
227.484101	5432.940373	15.862349	-0.046597	3.994762
227.332594	5424.873099	15.867354	-0.046564	3.991913
227.380205	5416.855483	15.872359	-0.046568	3.989083
227.436863	5408.910252	15.877363	-0.046573	3.986277
227.398376	5400.865586	15.882368	-0.046561	3.983432
227.453611	5392.944904	15.887373	-0.046567	3.980630
227.323372	5384.946833	15.892378	-0.046537	3.977796
227.299542	5376.943337	15.897383	-0.046528	3.974960
227.073011	5368.919090	15.902387	-0.046481	3.972111
227.172067	5360.888729	15.907392	-0.046494	3.969263
227.234292	5352.969562	15.912397	-0.046501	3.966452
226.989669	5344.949511	15.917402	-0.046450	3.963598
226.935480	5336.952502	15.922407	-0.046435	3.960753
226.835493	5329.001193	15.927411	-0.046412	3.957921
226.966948	5320.988301	15.932416	-0.046431	3.955070
227.025233	5312.967190	15.937421	-0.046437	3.952213
226.829392	5304.917044	15.942426	-0.046396	3.949338
226.799667	5296.951256	15.947431	-0.046385	3.946495
226.777216	5288.950674	15.952435	-0.046376	3.943637
226.546907	5280.965327	15.957440	-0.046328	3.940779
226.788784	5272.983346	15.962445	-0.046368	3.937928
226.702888	5264.980683	15.967450	-0.046347	3.935062
226.635295	5256.988204	15.972455	-0.046330	3.932198
226.680364	5248.955869	15.977459	-0.046333	3.929319
226.501106	5240.995540	15.982464	-0.046295	3.926460
226.346757	5233.006793	15.987469	-0.046261	3.923590
226.324491	5224.983367	15.992474	-0.046252	3.920707
226.268384	5217.032691	15.997479	-0.046237	3.917847
226.355206	5209.002455	16.002483	-0.046248	3.914960
226.129494	5200.953455	16.007488	-0.046201	3.912058
226.092365	5192.962286	16.012493	-0.046189	3.909178
226.129196	5184.993101	16.017498	-0.046191	3.906305
226.042444	5176.973065	16.022503	-0.046170	3.903409
226.003639	5169.011829	16.027507	-0.046157	3.900533
225.978242	5161.022105	16.032512	-0.046148	3.897646
226.106926	5153.000011	16.037517	-0.046167	3.894747
225.987142	5144.971092	16.042522	-0.046139	3.891839
225.961479	5136.952722	16.047527	-0.046130	3.888934
226.013204	5128.987042	16.052531	-0.046134	3.886048
225.815700	5120.977763	16.057536	-0.046093	3.883139
225.880441	5113.036181	16.062541	-0.046100	3.880257
225.581673	5105.028962	16.067546	-0.046039	3.877342
225.705537	5096.999082	16.072551	-0.046057	3.874425
225.652235	5088.763497	16.077555	-0.046042	3.871428
225.547750	5080.817371	16.082560	-0.046018	3.868533
225.676232	5072.897938	16.087565	-0.046037	3.865649
225.430601	5064.933811	16.092570	-0.045986	3.862740
225.455206	5056.969501	16.097575	-0.045986	3.859834
225.435198	5049.011936	16.102579	-0.045977	3.856928
225.303294	5040.988017	16.107584	-0.045948	3.853992
225.391852	5032.993018	16.112589	-0.045959	3.851070
225.278255	5024.955637	16.117594	-0.045933	3.848126
225.253247	5016.989368	16.122599	-0.045923	3.845207
225.341499	5009.029621	16.127603	-0.045935	3.842291
225.158953	5001.020526	16.132608	-0.045896	3.839348
225.071062	4993.093906	16.137613	-0.045875	3.836436
224.990384	4985.022611	16.142618	-0.045854	3.833469
224.998502	4977.000930	16.147623	-0.045851	3.830519
225.109440	4969.041468	16.152627	-0.045867	3.827592
224.988028	4960.998826	16.157632	-0.045839	3.824628
225.060611	4953.091885	16.162637	-0.045848	3.821715
225.059134	4945.034468	16.167642	-0.045842	3.818743
224.973506	4937.067662	16.172647	-0.045822	3.815800
224.795446	4929.071862	16.177651	-0.045783	3.812842
224.782405	4921.047420	16.182656	-0.045776	3.809875
224.768352	4913.110268	16.187661	-0.045768	3.806938
224.531722	4905.081896	16.192666	-0.045719	3.803960
224.407213	4897.123220	16.197671	-0.045691	3.801007
224.619203	4889.117280	16.202675	-0.045726	3.798043
224.552024	4881.059198	16.207680	-0.045708	3.795050
224.361228	4873.079537	16.212685	-0.045668	3.792082
224.488982	4865.030992	16.217690	-0.045687	3.789093
224.412207	4857.064721	16.222695	-0.045667	3.786127
224.262156	4849.083142	16.227699	-0.045634	3.783152
224.194567	4841.082016	16.232704	-0.045617	3.780169
224.382735	4833.101096	16.237709	-0.045647	3.777196
224.148492	4825.079209	16.242714	-0.045598	3.774197
224.125556	4817.082722	16.247719	-0.045589	3.771210
224.166854	4809.087004	16.252723	-0.045592	3.768222
223.962563	4801.055905	16.257728	-0.045549	3.765212
223.819766	4793.120067	16.262733	-0.045517	3.762238
223.924386	4785.087077	16.267738	-0.045532	3.759230
223.840197	4777.135368	16.272743	-0.045511	3.756246
223.945777	4769.105105	16.277747	-0.045526	3.753234
223.918666	4761.058746	16.282752	-0.045516	3.750211
223.926943	4753.118795	16.287757	-0.045512	3.747227
223.655256	4745.113909	16.292762	-0.045457	3.744209
223.791265	4737.132321	16.297767	-0.045477	3.741207
223.761827	4729.144299	16.302771	-0.045467	3.738196
223.644927	4721.145076	16.307776	-0.045440	3.735176
223.671450	4713.141655	16.312781	-0.045440	3.732156
223.377115	4705.110538	16.317786	-0.045380	3.729115
223.481112	4697.158161	16.322791	-0.045395	3.726111
223.525686	4689.147493	16.327795	-0.045398	3.723081
223.407439	4681.158702	16.332800	-0.045371	3.720053
223.558844	4673.216797	16.337805	-0.045394	3.717047
223.406530	4665.178226	16.342810	-0.045361	3.713994
223.237772	4657.092321	16.347815	-0.045324	3.710921
223.263704	4649.115575	16.352819	-0.045324	3.707891
223.328307	4641.108360	16.357824	-0.045331	3.704848
223.117408	4633.191263	16.362829	-0.045287	3.701830
223.181000	4625.166089	16.367834	-0.045294	3.698775
223.301695	4617.210912	16.372839	-0.045312	3.695746
223.297791	4609.210687	16.377843	-0.045306	3.692694
223.214850	4601.142196	16.382848	-0.045285	3.689611
223.119777	4593.224210	16.387853	-0.045263	3.686583
222.971794	4585.197968	16.392858	-0.045230	3.683510
222.928871	4577.253036	16.397863	-0.045217	3.680467
223.117595	4569.247918	16.402867	-0.045247	3.677406
222.840360	4561.211385	16.407872	-0.045191	3.674317
222.704164	4553.223508	16.412877	-0.045161	3.671249
222.569352	4545.229280	16.417882	-0.045130	3.668175
222.724791	4537.227909	16.422887	-0.045154	3.665104
222.594226	4529.270390	16.427891	-0.045125	3.662039
222.705339	4521.201061	16.432896	-0.045141	3.658935
222.712252	4513.254148	16.437901	-0.045137	3.655873
222.650824	4505.244118	16.442906	-0.045121	3.652782
222.635001	4497.206248	16.447911	-0.045113	3.649680
222.649941	4489.256316	16.452915	-0.045111	3.646609
222.434726	4481.270007	16.457920	-0.045066	3.643515
222.543117	4473.274690	16.462925	-0.045081	3.640424
222.295239	4465.323680	16.467930	-0.045030	3.637338
222.338956	4457.288444	16.472935	-0.045033	3.634224
222.249112	4449.268574	16.477939	-0.045011	3.631110
222.119138	4441.254414	16.482944	-0.044982	3.627995
222.075555	4433.243561	16.487949	-0.044969	3.624881
221.991062	4425.289022	16.492954	-0.044948	3.621784
221.881015	4417.292627	16.497959	-0.044923	3.618668
221.950280	4409.323353	16.502963	-0.044931	3.615565
221.847970	4401.309824	16.507968	-0.044907	3.612437
221.816452	4393.302261	16.512973	-0.044896	3.609310
221.631744	4385.319747	16.517978	-0.044857	3.606187
221.754282	4377.324704	16.522983	-0.044874	3.603064
221.745074	4369.320453	16.527987	-0.044868	3.599932
221.583996	4361.390643	16.532992	-0.044833	3.596821
221.689128	4353.368217	16.537997	-0.044847	3.593679
221.810285	4345.311047	16.543002	-0.044865	3.590521
221.570848	4337.373615	16.548007	-0.044815	3.587397
221.565223	4329.341300	16.553011	-0.044809	3.584240
221.601255	4321.405850	16.558016	-0.044811	3.581119
221.790175	4313.404339	16.563021	-0.044841	3.577974
221.665813	4305.381217	16.568026	-0.044813	3.574809
221.563072	4297.400861	16.573031	-0.044789	3.571658
221.485019	4289.402862	16.578035	-0.044770	3.568498
221.418974	4281.387409	16.583040	-0.044752	3.565329
221.570291	4273.433284	16.588045	-0.044776	3.562188
221.398650	4265.452486	16.593050	-0.044739	3.559024
221.356194	4257.478725	16.598055	-0.044726	3.555863
221.252257	4249.383664	16.603059	-0.044701	3.552650
221.334674	4241.286784	16.608064	-0.044712	3.549439
221.233576	4233.375891	16.613069	-0.044688	3.546293
220.915177	4225.416172	16.618074	-0.044624	3.543119
220.943991	4217.432125	16.623079	-0.044624	3.539942
220.942699	4209.456724	16.628083	-0.044619	3.536765
220.713209	4201.424351	16.633088	-0.044571	3.533556
220.721437	4193.423590	16.638093	-0.044568	3.530363
220.987405	4185.415164	16.643098	-0.044612	3.527172
220.674165	4177.440833	16.648103	-0.044549	3.523975
220.734751	4169.496019	16.653107	-0.044555	3.520798
220.604453	4161.499733	16.658112	-0.044526	3.517591
220.712411	4153.493289	16.663117	-0.044541	3.514385
220.643459	4145.485170	16.668122	-0.044523	3.511169
220.517070	4137.479532	16.673127	-0.044495	3.507950
220.408230	4129.475289	16.678131	-0.044470	3.504729
220.260283	4121.551293	16.683136	-0.044437	3.501536
220.412887	4113.551567	16.688141	-0.044461	3.498320
220.285536	4105.529085	16.693146	-0.044432	3.495082
220.222201	4097.517607	16.698151	-0.044415	3.491847
220.381375	4089.564154	16.703155	-0.044440	3.488640
220.482763	4081.519038	16.708160	-0.044454	3.485392
220.374705	4073.598132	16.713165	-0.044429	3.482183
220.093019	4065.628158	16.718170	-0.044371	3.478947
220.159727	4057.595837	16.723175	-0.044379	3.475693
220.242801	4049.573560	16.728179	-0.044389	3.472441
219.988712	4041.563280	16.733184	-0.044337	3.469180
220.053703	4033.587432	16.738189	-0.044344	3.465940
219.892494	4025.612542	16.743194	-0.044309	3.462690
219.844996	4017.582478	16.748199	-0.044295	3.459418
219.656331	4009.660164	16.753203	-0.044255	3.456182
219.685757	4001.598568	16.758208	-0.044256	3.452894
219.807396	3993.598330	16.763213	-0.044273	3.449630
219.785421	3985.618746	16.768218	-0.044264	3.446368
219.691145	3977.615226	16.773223	-0.044242	3.443089
219.656051	3969.656471	16.778227	-0.044230	3.439828
219.393908	3961.701696	16.783232	-0.044177	3.436558
219.378947	3953.679697	16.788237	-0.044169	3.433266
219.440147	3945.649297	16.793242	-0.044175	3.429970
219.517900	3937.627513	16.798247	-0.044185	3.426674
219.527473	3929.676643	16.803251	-0.044182	3.423402
219.348227	3921.667878	16.808256	-0.044143	3.420097
219.385509	3913.719441	16.813261	-0.044145	3.416821
219.311406	3905.700890	16.818266	-0.044126	3.413508
219.340856	3897.699697	16.823271	-0.044127	3.410204
219.121759	3889.751819	16.828275	-0.044081	3.406909
219.280034	3881.741081	16.833280	-0.044106	3.403599
219.193884	3873.788612	16.838285	-0.044085	3.400301
219.072944	3865.812959	16.843290	-0.044057	3.396989
219.108830	3857.754567	16.848295	-0.044059	3.393644
218.937723	3849.680971	16.853299	-0.044022	3.390283
218.881761	3841.696524	16.858304	-0.044007	3.386960
218.961581	3833.750434	16.863309	-0.044017	3.383654
219.079891	3825.757908	16.868314	-0.044034	3.380327
218.864377	3817.826969	16.873319	-0.043989	3.377010
218.910102	3809.809220	16.878323	-0.043992	3.373664
218.669190	3801.799223	16.883328	-0.043942	3.370306
218.697818	3793.860786	16.888333	-0.043943	3.366986
218.659101	3785.866659	16.893338	-0.043931	3.363636
218.727804	3777.855667	16.898343	-0.043938	3.360279
218.603878	3769.902683	16.903347	-0.043910	3.356937
218.496939	3761.849265	16.908352	-0.043885	3.353549
218.513651	3753.849740	16.913357	-0.043884	3.350186
218.358793	3745.856802	16.918362	-0.043850	3.346815
218.060024	3737.902260	16.923367	-0.043789	3.343452
218.290445	3729.900199	16.928371	-0.043827	3.340085
218.343082	3721.898699	16.933376	-0.043832	3.336708
218.325483	3713.911416	16.938381	-0.043824	3.333332
218.210985	3705.899430	16.943386	-0.043797	3.329937
218.344403	3697.894533	16.948391	-0.043817	3.326552
218.113263	3689.944521	16.953395	-0.043769	3.323173
218.095686	3681.943440	16.958400	-0.043761	3.319776
218.198683	3674.014820	16.963405	-0.043775	3.316412
218.039481	3665.975814	16.968410	-0.043741	3.312987
217.773037	3657.977442	16.973415	-0.043686	3.309572
217.750103	3649.995083	16.978419	-0.043677	3.306169
217.670515	3641.986510	16.983424	-0.043657	3.302749
217.694102	3634.028932	16.988429	-0.043657	3.299352
217.590171	3626.051545	16.993434	-0.043632	3.295938
217.694903	3618.016358	16.998439	-0.043647	3.292503
217.809933	3610.033016	17.003443	-0.043663	3.289088
217.502959	3602.072657	17.008448	-0.043601	3.285662
217.571971	3594.100607	17.013453	-0.043609	3.282243
217.577366	3586.085956	17.018458	-0.043605	3.278799
217.437325	3578.126282	17.023463	-0.043574	3.275369
217.493332	3570.089810	17.028467	-0.043579	3.271911
217.516343	3562.072056	17.033472	-0.043579	3.268456
217.403161	3554.103402	17.038477	-0.043553	3.265012
217.232957	3546.153484	17.043482	-0.043516	3.261571
217.316771	3538.136808	17.048487	-0.043527	3.258108
217.172700	3530.175498	17.053491	-0.043495	3.254655
216.864505	3522.167256	17.058496	-0.043433	3.251172
217.013391	3514.181687	17.063501	-0.043455	3.247714
216.885071	3506.174139	17.068506	-0.043426	3.244231
216.923925	3498.195655	17.073511	-0.043429	3.240764
217.078950	3490.207742	17.078515	-0.043453	3.237293
217.113105	3482.187286	17.083520	-0.043454	3.233800
216.811913	3474.183847	17.088525	-0.043393	3.230297
216.692748	3466.217973	17.093530	-0.043366	3.226814
216.772130	3458.202206	17.098535	-0.043376	3.223313
216.767374	3450.258619	17.103539	-0.043370	3.219837
216.750505	3442.249966	17.108544	-0.043362	3.216327
216.927340	3434.258149	17.113549	-0.043390	3.212830
216.905326	3426.237570	17.118554	-0.043381	3.209308
216.788667	3418.266704	17.123559	-0.043354	3.205799
216.857589	3410.320371	17.128563	-0.043362	3.202306
216.575629	3402.346569	17.133568	-0.043304	3.198782
216.386442	3394.401174	17.138573	-0.043264	3.195270
216.409408	3386.358864	17.143578	-0.043263	3.191721
216.560382	3378.337973	17.148583	-0.043287	3.188182
216.618491	3370.352435	17.153587	-0.043292	3.184652
216.269795	3362.403470	17.158592	-0.043223	3.181116
216.267267	3354.421807	17.163597	-0.043217	3.177576
216.315794	3346.411793	17.168602	-0.043221	3.174023
216.310586	3338.402573	17.173607	-0.043215	3.170463
216.019133	3330.468598	17.178611	-0.043156	3.166920
216.155571	3322.439152	17.183616	-0.043176	3.163350
216.119561	3314.480227	17.188621	-0.043165	3.159799
215.885876	3306.545998	17.193626	-0.043116	3.156247
215.865202	3298.486965	17.198631	-0.043108	3.152644
215.924924	3290.474633	17.203635	-0.043114	3.149062
215.856721	3282.476942	17.208640	-0.043096	3.145476
215.613249	3274.539679	17.213645	-0.043046	3.141906
215.775714	3266.529299	17.218650	-0.043071	3.138316
215.620689	3258.539119	17.223655	-0.043037	3.134718
215.421769	3250.575002	17.228659	-0.042995	3.131125
215.445699	3242.571794	17.233664	-0.042995	3.127520
215.377241	3234.586948	17.238669	-0.042977	3.123916
215.268120	3226.647863	17.243674	-0.042952	3.120326
215.341710	3218.648052	17.248679	-0.042960	3.116712
215.587004	3210.640387	17.253683	-0.043001	3.113099
215.296032	3202.606577	17.258688	-0.042942	3.109445
215.159461	3194.665958	17.263693	-0.042912	3.105837
215.222386	3186.681685	17.268698	-0.042918	3.102213
215.229130	3178.678044	17.273703	-0.042915	3.098574
215.235450	3170.720853	17.278707	-0.042911	3.094951
215.233670	3162.697813	17.283712	-0.042906	3.091294
215.155499	3154.733685	17.288717	-0.042886	3.087656
214.940015	3146.749165	17.293722	-0.042841	3.083998
214.814079	3138.778798	17.298727	-0.042813	3.080346
214.835440	3130.828204	17.303731	-0.042812	3.076706
214.691908	3122.773132	17.308736	-0.042780	3.073006
214.796569	3114.720899	17.313741	-0.042794	3.069314
214.901411	3106.744128	17.318746	-0.042809	3.065652
214.735453	3098.786226	17.323751	-0.042773	3.061982
214.401842	3090.853775	17.328755	-0.042706	3.058312
214.559386	3082.827163	17.333760	-0.042730	3.054617
214.384159	3074.868056	17.338765	-0.042693	3.050932
214.373865	3066.874668	17.343770	-0.042686	3.047236
214.227066	3058.914515	17.348775	-0.042654	3.043543
214.425927	3050.932383	17.353779	-0.042686	3.039853
214.217113	3042.973183	17.358784	-0.042642	3.036149
214.232356	3034.944142	17.363789	-0.042640	3.032419
214.050292	3026.962261	17.368794	-0.042601	3.028696
214.072058	3018.940916	17.373799	-0.042600	3.024961
214.111531	3010.995185	17.378803	-0.042602	3.021257
214.000490	3003.013454	17.383808	-0.042577	3.017524
213.986166	2995.048872	17.388813	-0.042569	3.013800
214.037420	2987.030610	17.393818	-0.042574	3.010049
213.809086	2979.072357	17.398823	-0.042526	3.006307
213.966620	2971.093445	17.403827	-0.042551	3.002570
213.726778	2963.107237	17.408832	-0.042501	2.998806
213.697940	2955.149984	17.413837	-0.042491	2.995061
213.680743	2947.115365	17.418842	-0.042482	2.991275
213.718007	2939.112267	17.423847	-0.042484	2.987502
213.459686	2931.165886	17.428851	-0.042431	2.983736
213.630648	2923.152932	17.433856	-0.042458	2.979956
213.674835	2915.200489	17.438861	-0.042462	2.976193
213.454075	2907.218619	17.443866	-0.042416	2.972398
213.316836	2899.214452	17.448871	-0.042385	2.968591
213.690758	2891.201226	17.453875	-0.042450	2.964802
213.396153	2883.262041	17.458880	-0.042390	2.961009
213.503260	2875.319393	17.463885	-0.042405	2.957230
213.276473	2867.330657	17.468890	-0.042358	2.953406
213.379934	2859.276860	17.473895	-0.042372	2.949564
213.351240	2851.323467	17.478899	-0.042362	2.945758
213.344630	2843.333029	17.483904	-0.042355	2.941931
213.079306	2835.418831	17.488909	-0.042301	2.938121
213.019224	2827.406293	17.493914	-0.042285	2.934270
212.856450	2819.407068	17.498919	-0.042250	2.930415
212.985410	2811.433244	17.503923	-0.042269	2.926582
212.945424	2803.450104	17.508928	-0.042256	2.922731
212.872704	2795.500482	17.513933	-0.042238	2.918890
212.900629	2787.508362	17.518938	-0.042238	2.915028
212.687039	2779.431566	17.523943	-0.042193	2.911107
212.564492	2771.481250	17.528947	-0.042166	2.907247
212.516386	2763.490272	17.533952	-0.042152	2.903366
212.798889	2755.502978	17.538957	-0.042199	2.899499
212.553344	2747.589165	17.543962	-0.042149	2.895635
212.337995	2739.580899	17.548967	-0.042104	2.891721
212.700346	2731.580118	17.553971	-0.042166	2.887837
212.459895	2723.618077	17.558976	-0.042116	2.883933
212.164300	2715.707529	17.563981	-0.042056	2.880047
212.104112	2707.702554	17.568986	-0.042040	2.876121
212.080627	2699.698073	17.573991	-0.042031	2.872193
212.087994	2691.711256	17.578995	-0.042027	2.868269
211.794895	2683.731059	17.584000	-0.041968	2.864327
211.890839	2675.751801	17.589005	-0.041981	2.860402
211.952237	2667.769631	17.594010	-0.041987	2.856467
211.812802	2659.793940	17.599015	-0.041956	2.852519
212.041460	2651.786479	17.604019	-0.041994	2.848571
211.891973	2643.815825	17.609024	-0.041961	2.844614
211.992080	2635.882107	17.614029	-0.041975	2.840684
211.914162	2627.912976	17.619034	-0.041955	2.836721
211.740068	2619.899494	17.624039	-0.041918	2.832725
211.785925	2611.911159	17.629043	-0.041921	2.828748
211.563047	2603.913450	17.634048	-0.041875	2.824746
211.817313	2595.940042	17.639053	-0.041917	2.820777
211.646467	2587.986532	17.644058	-0.041881	2.816788
211.645224	2579.996884	17.649063	-0.041875	2.812786
211.345786	2572.046685	17.654067	-0.041815	2.808780
211.378890	2564.034288	17.659072	-0.041816	2.804756
211.483913	2556.088315	17.664077	-0.041831	2.800764
211.359013	2548.121366	17.669082	-0.041802	2.796743
211.343960	2540.103146	17.674087	-0.041795	2.792696
211.310466	2532.136353	17.679091	-0.041783	2.788669
211.067585	2524.149927	17.684096	-0.041733	2.784613
211.123027	2516.207655	17.689101	-0.041739	2.780591
211.136104	2508.243669	17.694106	-0.041736	2.776550
211.071725	2500.246297	17.699111	-0.041719	2.772481
211.352535	2492.233817	17.704115	-0.041766	2.768420
211.043413	2484.273272	17.709120	-0.041704	2.764343
211.157221	2476.317187	17.714125	-0.041720	2.760288
211.077239	2468.361329	17.719130	-0.041700	2.756216
210.971432	2460.313689	17.724135	-0.041676	2.752089
210.926810	2452.322674	17.729139	-0.041662	2.747989
210.642348	2444.352495	17.734144	-0.041604	2.743878
210.782788	2436.399957	17.739149	-0.041626	2.739796
210.650646	2428.436372	17.744154	-0.041596	2.735686
210.404714	2420.438465	17.749159	-0.041545	2.731545
210.519608	2412.471519	17.754163	-0.041562	2.727436
210.364097	2404.500476	17.759168	-0.041528	2.723302
210.521788	2396.521730	17.764173	-0.041552	2.719177
210.433207	2388.597638	17.769178	-0.041531	2.715059
210.271576	2380.593533	17.774183	-0.041496	2.710888
210.304727	2372.635419	17.779187	-0.041497	2.706747
209.968748	2364.660775	17.784192	-0.041429	2.702568
209.981575	2356.700927	17.789197	-0.041427	2.698412
210.087515	2348.695003	17.794202	-0.041442	2.694231
210.136106	2340.696447	17.799207	-0.041446	2.690044
210.064115	2332.748067	17.804211	-0.041427	2.685869
209.941738	2324.786716	17.809216	-0.041400	2.681678
210.072594	2316.824974	17.814221	-0.041419	2.677496
209.981305	2308.858760	17.819226	-0.041397	2.673291
209.825181	2300.853335	17.824231	-0.041363	2.669055
209.986437	2292.851561	17.829235	-0.041388	2.664834
209.689890	2284.913484	17.834240	-0.041328	2.660610
209.638492	2276.957060	17.839245	-0.041313	2.656386
209.565991	2268.967170	17.844250	-0.041295	2.652136
209.561061	2260.975692	17.849255	-0.041289	2.647883
209.500738	2253.031941	17.854259	-0.041273	2.643645
209.670586	2245.038198	17.859264	-0.041300	2.639388
209.682605	2237.091843	17.864269	-0.041297	2.635139
209.574542	2229.105249	17.869274	-0.041272	2.630854
209.402544	2221.151541	17.874279	-0.041235	2.626576
209.594374	2213.156893	17.879283	-0.041266	2.622293
209.496116	2205.190842	17.884288	-0.041242	2.617998
209.394060	2197.246774	17.889293	-0.041218	2.613708
209.394978	2189.253621	17.894298	-0.041214	2.609392
209.194137	2181.299664	17.899303	-0.041171	2.605076
209.176630	2173.353422	17.904307	-0.041163	2.600769
209.188719	2165.372396	17.909312	-0.041160	2.596439
209.178982	2157.287195	17.914317	-0.041154	2.592043
208.807081	2149.283974	17.919322	-0.041079	2.587659
208.912905	2141.318679	17.924327	-0.041094	2.583321
208.888440	2133.399329	17.929331	-0.041085	2.578992
208.699499	2125.450999	17.934336	-0.041045	2.574629
208.995865	2117.462787	17.939341	-0.041095	2.570270
208.988373	2109.499876	17.944346	-0.041088	2.565896
208.792983	2101.567764	17.949351	-0.041047	2.561519
208.800740	2093.619083	17.954355	-0.041044	2.557139
208.564571	2085.661248	17.959360	-0.040995	2.552730
208.579546	2077.686262	17.964365	-0.040993	2.548321
208.358934	2069.737279	17.969370	-0.040947	2.543902
208.333560	2061.763319	17.974375	-0.040937	2.539476
208.329114	2053.820805	17.979379	-0.040931	2.535061
208.052129	2045.840109	17.984384	-0.040875	2.530597
208.099731	2037.862332	17.989389	-0.040878	2.526150
208.264753	2029.881292	17.994394	-0.040904	2.521702
208.122212	2021.950901	17.999399	-0.040873	2.517252
208.051628	2013.982261	18.004403	-0.040855	2.512779
207.775298	2005.990198	18.009408	-0.040798	2.508269
207.956214	1997.996418	18.014413	-0.040827	2.503783
207.828677	1990.060807	18.019418	-0.040798	2.499299
207.919031	1982.072962	18.024423	-0.040810	2.494794
207.976344	1974.120298	18.029427	-0.040816	2.490298
207.786762	1966.160314	18.034432	-0.040776	2.485772
207.703103	1958.225901	18.039437	-0.040755	2.481260
207.711611	1950.261088	18.044442	-0.040752	2.476729
207.810905	1942.282598	18.049447	-0.040765	2.472189
207.559310	1934.334689	18.054451	-0.040714	2.467631
207.480963	1926.360721	18.059456	-0.040694	2.463063
207.483455	1918.415772	18.064461	-0.040689	2.458510
207.406311	1910.450068	18.069466	-0.040670	2.453930
207.176491	1902.489486	18.074471	-0.040622	2.449333
207.162896	1894.548588	18.079475	-0.040615	2.444755
207.096667	1886.574399	18.084480	-0.040598	2.440145
207.108165	1878.623668	18.089485	-0.040595	2.435545
206.872291	1870.607591	18.094490	-0.040546	2.430881
206.758147	1862.625324	18.099495	-0.040520	2.426236
206.963048	1854.661474	18.104499	-0.040553	2.421618
206.890333	1846.706674	18.109504	-0.040535	2.416974
206.778959	1838.756311	18.114509	-0.040509	2.412321
206.710470	1830.795398	18.119514	-0.040491	2.407657
206.774994	1822.825592	18.124519	-0.040498	2.402988
206.824495	1814.900565	18.129523	-0.040502	2.398336
206.622340	1806.958773	18.134528	-0.040460	2.393645
206.411979	1799.000192	18.139533	-0.040416	2.388934
206.431097	1791.031727	18.144538	-0.040414	2.384226
206.422025	1783.070907	18.149543	-0.040408	2.379511
206.312182	1775.143597	18.154547	-0.040382	2.374798
206.195002	1767.157007	18.159552	-0.040356	2.370041
206.199495	1759.209139	18.164557	-0.040352	2.365306
206.273001	1751.259244	18.169562	-0.040360	2.360566
205.933891	1743.344736	18.174567	-0.040292	2.355805
206.156255	1735.331487	18.179571	-0.040329	2.351020
206.057133	1727.346513	18.184576	-0.040305	2.346217
206.080571	1719.397600	18.189581	-0.040305	2.341435
205.940821	1711.478010	18.194586	-0.040274	2.336648
205.973605	1703.482626	18.199591	-0.040275	2.331819
206.158014	1695.512478	18.204595	-0.040304	2.327008
205.758907	1687.606134	18.209600	-0.040225	2.322177
205.826166	1679.667421	18.214605	-0.040233	2.317356
205.901728	1671.698997	18.219610	-0.040242	2.312506
205.512461	1663.769515	18.224615	-0.040164	2.307632
205.678268	1655.799766	18.229619	-0.040190	2.302769
205.635290	1647.840564	18.234624	-0.040177	2.297885
205.570045	1639.896035	18.239629	-0.040160	2.292998
205.474617	1631.940728	18.244634	-0.040138	2.288090
205.501850	1623.981580	18.249639	-0.040138	2.283181
205.429677	1616.062828	18.254643	-0.040119	2.278277
205.187677	1608.097857	18.259648	-0.040069	2.273319
205.141550	1600.087892	18.264653	-0.040056	2.268340
205.242404	1592.123990	18.269658	-0.040070	2.263391
204.960193	1584.217877	18.274663	-0.040012	2.258434
204.976803	1576.277520	18.279667	-0.040010	2.253470
204.807715	1568.312069	18.284672	-0.039974	2.248464
204.908656	1560.356844	18.289677	-0.039988	2.243476
204.798063	1552.445545	18.294682	-0.039962	2.238486
204.787990	1544.482527	18.299687	-0.039955	2.233462
204.942013	1536.496441	18.304691	-0.039979	2.228426
204.681869	1528.580700	18.309696	-0.039926	2.223386
204.834015	1520.629355	18.314701	-0.039949	2.218350
204.819284	1512.694918	18.319706	-0.039941	2.213297
204.522100	1504.762893	18.324711	-0.039881	2.208209
204.567304	1496.830325	18.329715	-0.039885	2.203140
204.497461	1488.881860	18.334720	-0.039867	2.198038
204.434392	1480.944129	18.339725	-0.039850	2.192933
204.392150	1472.969429	18.344730	-0.039837	2.187793
204.241260	1465.032749	18.349735	-0.039804	2.182656
204.269754	1457.102633	18.354739	-0.039805	2.177527
204.268020	1449.133681	18.359744	-0.039799	2.172358
204.122763	1441.197391	18.364749	-0.039767	2.167185
204.222918	1433.249706	18.369754	-0.039781	2.162015
204.108046	1425.333252	18.374759	-0.039755	2.156833
203.935188	1417.415843	18.379763	-0.039718	2.151632
203.946363	1409.452635	18.384768	-0.039715	2.146405
204.063328	1401.500270	18.389773	-0.039732	2.141184
203.943431	1393.589840	18.394778	-0.039704	2.135954
203.758176	1385.647412	18.399783	-0.039665	2.130685
203.705178	1377.721715	18.404787	-0.039650	2.125426
203.533653	1369.794020	18.409792	-0.039613	2.120141
203.518481	1361.865750	18.414797	-0.039606	2.114857
203.592510	1353.833755	18.419802	-0.039614	2.109500
203.290687	1345.928602	18.424807	-0.039553	2.104178
203.353409	1337.998523	18.429811	-0.039560	2.098861
203.445699	1330.037622	18.434816	-0.039572	2.093512
203.468114	1322.092795	18.439821	-0.039571	2.088154
203.270184	1314.197825	18.444826	-0.039530	2.082794
203.280250	1306.263140	18.449831	-0.039527	2.077413
203.368027	1298.334212	18.454835	-0.039538	2.072031
203.133406	1290.416607	18.459840	-0.039489	2.066610
203.094836	1282.489224	18.464845	-0.039477	2.061187
203.136989	1274.556336	18.469850	-0.039480	2.055755
203.002369	1266.627162	18.474855	-0.039450	2.050293
202.832777	1258.715731	18.479859	-0.039414	2.044825
202.755538	1250.795979	18.484864	-0.039394	2.039345
202.680732	1242.877158	18.489869	-0.039376	2.033852
202.699113	1234.905889	18.494874	-0.039374	2.028318
202.427450	1227.002702	18.499879	-0.039319	2.022785
202.537938	1219.070907	18.504883	-0.039334	2.017257
202.688315	1211.097191	18.509888	-0.039357	2.011689
202.466328	1203.196553	18.514893	-0.039311	2.006117
202.577866	1195.260369	18.519898	-0.039327	2.000540
202.326488	1187.385070	18.524903	-0.039275	1.994952
202.310439	1179.445299	18.529907	-0.039267	1.989328
202.322316	1171.506031	18.534912	-0.039265	1.983691
202.265067	1163.604848	18.539917	-0.039249	1.978057
201.992132	1155.716913	18.544922	-0.039193	1.972394
201.855086	1147.781034	18.549927	-0.039163	1.966695
202.110812	1139.839419	18.554931	-0.039206	1.961018
201.882579	1131.960612	18.559936	-0.039158	1.955316
201.691346	1124.004911	18.564941	-0.039118	1.949547
201.817485	1116.054900	18.569946	-0.039136	1.943799
201.696118	1108.152837	18.574951	-0.039109	1.938042
201.608791	1100.244611	18.579955	-0.039087	1.932267
201.645050	1092.300298	18.584960	-0.039089	1.926462
201.676911	1084.407520	18.589965	-0.039090	1.920676
201.494556	1076.512367	18.594970	-0.039051	1.914848
201.174705	1068.619514	18.599975	-0.038987	1.908988
201.489740	1060.660405	18.604979	-0.039041	1.903132
201.228012	1052.781720	18.609984	-0.038987	1.897253
201.253895	1044.849006	18.614989	-0.038987	1.891347
201.316864	1036.923269	18.619994	-0.038994	1.885433
201.089039	1029.062853	18.624999	-0.038946	1.879516
201.216066	1021.143391	18.630003	-0.038965	1.873576
201.082939	1013.218153	18.635008	-0.038936	1.867583
200.975906	1005.326181	18.640013	-0.038911	1.861600
200.880769	997.434004	18.645018	-0.038888	1.855597
200.730709	989.522414	18.650023	-0.038855	1.849555
200.728693	981.626498	18.655027	-0.038850	1.843521
200.714904	973.718558	18.660032	-0.038842	1.837458
200.636388	965.822944	18.665037	-0.038823	1.831376
200.544950	957.921650	18.670042	-0.038801	1.825268
200.639965	950.012861	18.675047	-0.038814	1.819155
200.293257	942.173449	18.680051	-0.038744	1.813023
200.038898	934.273988	18.685056	-0.038692	1.806835
200.444682	926.322914	18.690061	-0.038763	1.800664
200.226583	918.471732	18.695066	-0.038717	1.794476
200.067974	910.525000	18.700071	-0.038683	1.788197
200.237901	902.616946	18.705075	-0.038709	1.781967
200.376139	894.698444	18.710080	-0.038730	1.775704
200.205902	886.836755	18.715085	-0.038694	1.769425
199.999647	878.988606	18.720090	-0.038650	1.763130
199.842745	871.126717	18.725095	-0.038616	1.756808
199.899873	863.219300	18.730099	-0.038622	1.750453
199.755750	855.340536	18.735104	-0.038590	1.744072
199.940408	847.441484	18.740109	-0.038620	1.737694
199.789748	839.559259	18.745114	-0.038587	1.731262
199.448552	831.716686	18.750119	-0.038518	1.724815
199.511696	823.849255	18.755123	-0.038525	1.718375
199.464936	815.956536	18.760128	-0.038512	1.711876
199.362961	808.071541	18.765133	-0.038488	1.705352
199.533043	800.175334	18.770138	-0.038515	1.698828
199.551518	792.286008	18.775143	-0.038513	1.692266
199.342199	784.444971	18.780147	-0.038469	1.685687
199.115059	776.609648	18.785152	-0.038422	1.679086
199.240746	768.717716	18.790157	-0.038441	1.672458
199.158299	760.856203	18.795162	-0.038420	1.665801
198.888399	753.021792	18.800167	-0.038365	1.659115
199.056173	745.126301	18.805171	-0.038392	1.652410
199.039527	737.248860	18.810176	-0.038384	1.645667
198.985834	729.409202	18.815181	-0.038369	1.638924
198.754217	721.557991	18.820186	-0.038321	1.632119
198.575978	713.665895	18.825191	-0.038283	1.625257
198.583625	705.823501	18.830195	-0.038279	1.618435
198.379099	697.979108	18.835200	-0.038236	1.611553
198.335985	690.122407	18.840205	-0.038223	1.604653
198.514985	682.253181	18.845210	-0.038252	1.597743
198.351899	674.410457	18.850215	-0.038217	1.590779
198.356322	666.572575	18.855219	-0.038213	1.583812
198.268400	658.736890	18.860224	-0.038191	1.576803
198.173734	650.897211	18.865229	-0.038169	1.569758
198.138171	643.065047	18.870234	-0.038157	1.562697
198.131619	635.226377	18.875239	-0.038151	1.555602
198.137625	627.369970	18.880243	-0.038148	1.548460
197.766704	619.573339	18.885248	-0.038074	1.541283
197.675862	611.756335	18.890253	-0.038052	1.534097
197.738643	603.899150	18.895258	-0.038059	1.526862
197.548219	596.101259	18.900263	-0.038018	1.519609
197.421281	588.297587	18.905267	-0.037990	1.512326
197.500413	580.428522	18.910272	-0.038000	1.504978
197.532150	572.612233	18.915277	-0.038001	1.497637
197.487401	564.792243	18.920282	-0.037988	1.490243
197.175453	557.017682	18.925287	-0.037925	1.482815
197.316387	549.193445	18.930291	-0.037946	1.475372
197.004306	541.359664	18.935296	-0.037883	1.467811
197.076030	533.540953	18.940301	-0.037892	1.460287
197.184207	525.722928	18.945306	-0.037907	1.452730
196.892331	517.947263	18.950311	-0.037848	1.445110
197.019016	510.148322	18.955315	-0.037866	1.437495
196.821206	502.372492	18.960320	-0.037825	1.429809
196.949111	494.554122	18.965325	-0.037844	1.422093
196.760242	486.802448	18.970330	-0.037804	1.414349
196.493098	479.033961	18.975335	-0.037749	1.406532
196.652689	471.242165	18.980339	-0.037774	1.398720
196.483354	463.467230	18.985344	-0.037738	1.390825
196.355289	455.693575	18.990349	-0.037709	1.382894
196.498301	447.904106	18.995354	-0.037731	1.374947
196.315229	440.135322	19.000359	-0.037692	1.366919
196.315910	432.386014	19.005363	-0.037687	1.358895
196.284748	424.621154	19.010368	-0.037677	1.350802
196.281531	416.858850	19.015373	-0.037671	1.342668
196.214181	409.130034	19.020378	-0.037654	1.334508
196.033862	401.386807	19.025383	-0.037616	1.326263
196.124833	393.645480	19.030387	-0.037628	1.318016
195.718059	385.867877	19.035392	-0.037547	1.309589
195.833860	378.071958	19.040397	-0.037564	1.301182
195.559131	370.397566	19.045402	-0.037508	1.292782
195.333826	362.685271	19.050407	-0.037461	1.284294
195.346237	354.975085	19.055411	-0.037459	1.275796
195.225927	347.261239	19.060416	-0.037432	1.267212
195.163674	339.562008	19.065421	-0.037415	1.258597
195.120167	331.862595	19.070426	-0.037402	1.249925
194.877945	324.189245	19.075431	-0.037352	1.241185
195.089965	316.463140	19.080435	-0.037387	1.232410
194.889361	308.778308	19.085440	-0.037345	1.223539
194.678310	301.129060	19.090445	-0.037301	1.214643
194.901719	293.401082	19.095450	-0.037338	1.205675
194.600043	285.786848	19.100455	-0.037277	1.196669
194.489137	278.137203	19.105459	-0.037252	1.187591
194.539974	270.455383	19.110464	-0.037256	1.178437
194.681204	262.782177	19.115469	-0.037278	1.169241
194.452602	255.184743	19.120474	-0.037230	1.159987
194.360235	247.530195	19.125479	-0.037209	1.150618
194.495854	239.861845	19.130483	-0.037229	1.141202
194.194912	232.288847	19.135488	-0.037168	1.131734
194.120095	224.683748	19.140493	-0.037150	1.122194
193.867904	217.126836	19.145498	-0.037098	1.112595
193.754701	209.526857	19.150503	-0.037072	1.102887
193.670074	201.955102	19.155507	-0.037052	1.093137
193.658167	194.366501	19.160512	-0.037045	1.083292
193.810461	186.773294	19.165517	-0.037069	1.073389
193.726545	179.211550	19.170522	-0.037048	1.063381
193.290888	171.729181	19.175527	-0.036962	1.053303
193.380095	164.177627	19.180531	-0.036974	1.043156
193.126454	156.686800	19.185536	-0.036923	1.032912
193.084006	149.163769	19.190541	-0.036910	1.022571
193.157806	141.646516	19.195546	-0.036919	1.012160
192.924527	134.183937	19.200551	-0.036871	1.001643
192.923845	126.696624	19.205555	-0.036866	0.991037
192.576838	119.253256	19.210560	-0.036797	0.980293
192.761511	111.758048	19.215565	-0.036827	0.969489
192.663277	104.338806	19.220570	-0.036804	0.958602
192.273325	96.967955	19.225575	-0.036727	0.947586
192.283347	89.558599	19.230579	-0.036724	0.936488
192.145631	82.173564	19.235584	-0.036694	0.925254
191.864953	74.847671	19.240589	-0.036637	0.913935
191.924278	67.457557	19.245594	-0.036643	0.902466
191.717377	60.374099	19.250599	-0.036601	0.891262