Thu Mar 11 18:30:30 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.594305	0.006745	0.000000	0.000005	0.724603

0.461896	0.024672	0.005005	0.000029	0.724592
0.510302	0.017228	0.010010	0.000020	0.724595
0.468211	0.025296	0.015014	0.000028	0.724597
0.554252	0.007244	0.020019	0.000012	0.724592
0.566931	0.009709	0.025024	0.000009	0.724601
0.381164	0.037733	0.030029	0.000043	0.724592
0.378007	0.040824	0.035034	0.000044	0.724597
0.597979	0.001839	0.040038	0.000002	0.724598
0.514137	0.013592	0.045043	0.000018	0.724592
0.427591	0.032725	0.050048	0.000034	0.724600
0.524904	0.010792	0.055053	0.000015	0.724591
0.473681	0.022281	0.060058	0.000025	0.724597
0.372399	0.039292	0.065062	0.000043	0.724595
0.290132	0.052120	0.070067	0.000058	0.724592
0.518387	0.016246	0.075072	0.000016	0.724602
0.391588	0.026754	0.080077	0.000039	0.724578
0.444821	-0.144255	0.085082	0.000029	0.724263
0.507954	-0.155598	0.090086	0.000017	0.724263
0.463349	-0.149992	0.095091	0.000025	0.724259
0.425378	-0.139109	0.100096	0.000032	0.724267
0.390498	-0.137865	0.105101	0.000038	0.724258
0.557752	-0.166509	0.110106	0.000007	0.724261
0.392831	-0.220668	0.115110	0.000037	0.724097
0.219051	-0.266139	0.120115	0.000069	0.723948
0.438491	-0.301007	0.125120	0.000028	0.723957
0.239870	-0.271206	0.130125	0.000065	0.723946
0.436139	-0.303862	0.135130	0.000028	0.723951
0.525933	-0.382699	0.140134	0.000011	0.723829
0.505392	-0.480913	0.145139	0.000015	0.723629
0.242596	-0.429807	0.150144	0.000064	0.723638
0.310360	-0.446794	0.155149	0.000051	0.723629
0.471620	-0.492294	0.160154	0.000021	0.723597
0.302191	-0.591595	0.165158	0.000052	0.723343
0.178018	-0.571580	0.170163	0.000075	0.723340
0.212617	-0.572469	0.175168	0.000068	0.723350
0.288805	-0.639399	0.180173	0.000054	0.723246
0.351204	-0.771279	0.185178	0.000042	0.723010
0.289134	-0.762359	0.190182	0.000053	0.723006
0.285658	-0.763475	0.195187	0.000054	0.723003
0.289392	-0.897001	0.200192	0.000053	0.722743
0.153399	-0.900295	0.205197	0.000078	0.722689
0.190157	-0.904079	0.210202	0.000071	0.722695
0.180956	-1.012462	0.215206	0.000073	0.722480
0.273061	-1.086377	0.220211	0.000055	0.722367
0.424530	-1.108481	0.225216	0.000027	0.722377
0.382923	-1.220187	0.230221	0.000034	0.722144
0.233092	-1.228147	0.235226	0.000062	0.722076
0.252706	-1.235796	0.240230	0.000058	0.722068
0.198114	-1.392052	0.245235	0.000068	0.721743
0.125751	-1.375815	0.250240	0.000082	0.721750
0.223640	-1.458328	0.255245	0.000063	0.721622
0.277912	-1.560500	0.260250	0.000053	0.721441
0.265668	-1.558264	0.265254	0.000055	0.721442
0.062525	-1.675501	0.270259	0.000093	0.721140
0.040684	-1.677549	0.275264	0.000096	0.721129
-0.027283	-1.733607	0.280269	0.000109	0.720996
0.082999	-1.812825	0.285274	0.000088	0.720879
-0.182901	-1.793546	0.290278	0.000137	0.720824
-0.370971	-1.905839	0.295283	0.000172	0.720538
-2.147650	-1.587450	0.300288	0.000503	0.720542
-1.979342	-1.693771	0.305293	0.000471	0.720392
-3.155878	-1.570332	0.310298	0.000690	0.720223
-2.906057	-1.613775	0.315302	0.000643	0.720225
-3.140424	-1.577016	0.320307	0.000687	0.720216
-3.879836	-1.597128	0.325312	0.000824	0.719918
-4.270989	-1.541001	0.330317	0.000897	0.719891
-3.924689	-1.599608	0.335322	0.000832	0.719898
-3.851289	-1.611832	0.340326	0.000818	0.719900
-5.104233	-1.529447	0.345331	0.001051	0.719623
-5.138129	-1.532305	0.350336	0.001057	0.719606
-4.947039	-1.570835	0.355341	0.001021	0.719597
-5.110625	-1.540539	0.360346	0.001052	0.719600
-5.150117	-1.556496	0.365350	0.001059	0.719555
-5.872073	-1.575131	0.370355	0.001193	0.719266
-5.737125	-1.593727	0.375360	0.001168	0.719277
-6.561628	-1.453085	0.380365	0.001321	0.719265
-5.996985	-1.551890	0.385370	0.001215	0.719269
-5.645339	-1.625069	0.390374	0.001150	0.719248
-7.046873	-1.523237	0.395379	0.001410	0.718957
-6.758399	-1.571592	0.400384	0.001356	0.718964
-6.933461	-1.541744	0.405389	0.001389	0.718962
-6.992919	-1.529993	0.410394	0.001400	0.718964
-7.014239	-1.524598	0.415398	0.001403	0.718968
-7.267559	-1.534889	0.420403	0.001450	0.718859
-8.151199	-1.484792	0.425408	0.001615	0.718648
-8.272464	-1.466976	0.430413	0.001637	0.718641
-8.216876	-1.475240	0.435418	0.001626	0.718644
-7.949866	-1.522742	0.440422	0.001576	0.718645
-8.277315	-1.467096	0.445427	0.001637	0.718640
-8.136288	-1.487809	0.450432	0.001611	0.718649
-8.092834	-1.585760	0.455437	0.001602	0.718472
-9.233123	-1.443132	0.460442	0.001814	0.718353
-8.775731	-1.522804	0.465446	0.001729	0.718357
-8.536653	-1.569798	0.470451	0.001684	0.718348
-8.513248	-1.568458	0.475456	0.001680	0.718360
-8.977373	-1.490799	0.480461	0.001766	0.718350
-9.037328	-1.531525	0.485466	0.001777	0.718249
-9.775230	-1.515976	0.490470	0.001914	0.718021
-9.806147	-1.515868	0.495475	0.001920	0.718010
-10.099854	-1.458088	0.500480	0.001974	0.718022
-9.847665	-1.509155	0.505485	0.001927	0.718010
-9.788275	-1.515886	0.510490	0.001916	0.718018
-10.011830	-1.475619	0.515494	0.001957	0.718019
-9.823667	-1.569955	0.520499	0.001922	0.717900
-10.601016	-1.527613	0.525504	0.002066	0.717710
-10.710102	-1.514487	0.530509	0.002086	0.717698
-10.703892	-1.514117	0.535514	0.002085	0.717701
-10.641022	-1.524235	0.540518	0.002073	0.717704
-10.852860	-1.488898	0.545523	0.002112	0.717700
-10.852281	-1.485393	0.550528	0.002112	0.717707
-10.714984	-1.594883	0.555533	0.002086	0.717540
-11.770904	-1.487081	0.560538	0.002282	0.717381
-11.961012	-1.452809	0.565542	0.002317	0.717383
-11.952911	-1.459645	0.570547	0.002316	0.717372
-11.575003	-1.524024	0.575552	0.002245	0.717379
-11.778830	-1.489756	0.580557	0.002283	0.717375
-12.093804	-1.431783	0.585562	0.002341	0.717379
-11.702314	-1.504856	0.590566	0.002268	0.717373
-12.074044	-1.587201	0.595571	0.002337	0.717080
-12.513135	-1.505305	0.600576	0.002419	0.717087
-12.735320	-1.469304	0.605581	0.002460	0.717081
-12.667345	-1.480057	0.610586	0.002447	0.717084
-12.597242	-1.491701	0.615590	0.002434	0.717086
-12.662323	-1.485302	0.620595	0.002446	0.717076
-12.223180	-1.578620	0.625600	0.002364	0.717047
-13.504020	-1.501361	0.630605	0.002602	0.716749
-13.475110	-1.505708	0.635610	0.002596	0.716751
-13.460552	-1.504699	0.640614	0.002593	0.716758
-13.690956	-1.468021	0.645619	0.002636	0.716750
-13.814161	-1.441959	0.650624	0.002659	0.716759
-13.672588	-1.470633	0.655629	0.002632	0.716752
-13.451226	-1.509498	0.660634	0.002591	0.716754
-13.710031	-1.564714	0.665638	0.002639	0.716554
-15.099940	-1.372813	0.670643	0.002897	0.716444
-14.232511	-1.523492	0.675648	0.002735	0.716452
-14.447119	-1.490019	0.680653	0.002775	0.716443
-14.912338	-1.404770	0.685658	0.002861	0.716448
-14.322391	-1.510238	0.690662	0.002751	0.716448
-14.500089	-1.481409	0.695667	0.002784	0.716443
-14.512890	-1.503354	0.700672	0.002786	0.716395
-15.441482	-1.474347	0.705677	0.002959	0.716125
-15.173490	-1.519709	0.710682	0.002909	0.716130
-15.564268	-1.448823	0.715686	0.002981	0.716133
-15.410781	-1.480524	0.720691	0.002953	0.716125
-14.975713	-1.552771	0.725696	0.002871	0.716136
-15.528034	-1.459373	0.730701	0.002974	0.716127
-15.593278	-1.445806	0.735706	0.002986	0.716131
-15.487827	-1.574362	0.740710	0.002966	0.715914
-16.182108	-1.468589	0.745715	0.003095	0.715879
-16.232871	-1.455791	0.750720	0.003104	0.715887
-16.205617	-1.464020	0.755725	0.003099	0.715880
-16.159492	-1.471868	0.760730	0.003090	0.715882
-16.365184	-1.433480	0.765734	0.003128	0.715886
-16.421643	-1.427819	0.770739	0.003138	0.715877
-16.762605	-1.519996	0.775744	0.003202	0.715575
-17.065851	-1.479346	0.780749	0.003258	0.715548
-17.376100	-1.424890	0.785754	0.003316	0.715547
-16.929287	-1.503213	0.790758	0.003232	0.715550
-17.325695	-1.437149	0.795763	0.003306	0.715542
-17.269080	-1.443284	0.800768	0.003295	0.715550
-17.379989	-1.428512	0.805773	0.003315	0.715541
-17.253125	-1.548195	0.810778	0.003292	0.715348
-17.976233	-1.478190	0.815782	0.003426	0.715232
-18.003722	-1.476821	0.820787	0.003431	0.715226
-17.773831	-1.513079	0.825792	0.003388	0.715235
-18.408532	-1.403143	0.830797	0.003506	0.715230
-18.131664	-1.452493	0.835802	0.003454	0.715230
-17.882922	-1.495690	0.840806	0.003407	0.715233
-18.344084	-1.523358	0.845811	0.003493	0.715015
-19.229692	-1.418236	0.850816	0.003658	0.714911
-19.004589	-1.460960	0.855821	0.003615	0.714906
-18.796027	-1.498221	0.860826	0.003576	0.714907
-18.995108	-1.461404	0.865830	0.003613	0.714910
-19.309453	-1.410148	0.870835	0.003672	0.714901
-19.020953	-1.456773	0.875840	0.003618	0.714911
-18.982753	-1.489874	0.880845	0.003610	0.714859
-19.896369	-1.451417	0.885850	0.003780	0.714613
-19.625380	-1.499800	0.890854	0.003729	0.714613
-20.053089	-1.427637	0.895859	0.003809	0.714605
-19.819412	-1.465874	0.900864	0.003765	0.714613
-19.920998	-1.451025	0.905869	0.003784	0.714606
-20.288092	-1.385180	0.910874	0.003852	0.714608
-19.668016	-1.493474	0.915878	0.003736	0.714613
-20.269244	-1.541118	0.920883	0.003848	0.714306
-20.910620	-1.440079	0.925888	0.003967	0.714280
-21.200147	-1.392020	0.930893	0.004021	0.714273
-21.186569	-1.393679	0.935898	0.004018	0.714275
-20.894061	-1.443972	0.940902	0.003963	0.714279
-20.871298	-1.450961	0.945907	0.003959	0.714274
-20.865045	-1.448290	0.950912	0.003957	0.714282
-21.083704	-1.443777	0.955917	0.003998	0.714214
-21.740424	-1.451593	0.960922	0.004120	0.713966
-21.568245	-1.479586	0.965926	0.004088	0.713972
-22.315503	-1.351897	0.970931	0.004227	0.713962
-21.738219	-1.449865	0.975936	0.004119	0.713972
-21.513266	-1.493819	0.980941	0.004077	0.713965
-21.812776	-1.438677	0.985946	0.004132	0.713969
-21.879112	-1.425785	0.990950	0.004144	0.713971
-22.254643	-1.507403	0.995955	0.004214	0.713676
-22.633620	-1.451214	1.000960	0.004284	0.713654
-22.754283	-1.433079	1.005965	0.004307	0.713648
-22.638737	-1.454595	1.010970	0.004285	0.713647
-22.840048	-1.416830	1.015974	0.004322	0.713651
-22.896061	-1.409546	1.020979	0.004332	0.713646
-22.519305	-1.473126	1.025984	0.004262	0.713653
-22.765968	-1.520539	1.030989	0.004308	0.713472
-24.110636	-1.340671	1.035994	0.004558	0.713354
-23.293980	-1.483141	1.040998	0.004406	0.713360
-23.555479	-1.440264	1.046003	0.004454	0.713353
-23.903152	-1.375050	1.051008	0.004518	0.713360
-23.695945	-1.416075	1.056013	0.004480	0.713353
-23.628539	-1.427954	1.061018	0.004467	0.713353
-23.471821	-1.509851	1.066022	0.004438	0.713246
-25.003999	-1.353811	1.071027	0.004723	0.713014
-24.604766	-1.420697	1.076032	0.004648	0.713023
-24.621767	-1.419969	1.081037	0.004651	0.713019
-24.570267	-1.428975	1.086042	0.004641	0.713020
-24.643930	-1.413484	1.091046	0.004655	0.713025
-24.958760	-1.361259	1.096051	0.004713	0.713018
-24.383707	-1.459079	1.101056	0.004606	0.713027
-24.432486	-1.552878	1.106061	0.004615	0.712824
-25.842546	-1.359527	1.111066	0.004877	0.712709
-25.371008	-1.441651	1.116070	0.004789	0.712713
-25.676273	-1.391127	1.121075	0.004845	0.712706
-25.594402	-1.400450	1.126080	0.004830	0.712717
-25.570690	-1.410268	1.131085	0.004825	0.712706
-25.598179	-1.405828	1.136090	0.004830	0.712706
-25.562500	-1.447529	1.141094	0.004823	0.712636
-26.245861	-1.451746	1.146099	0.004950	0.712385
-26.104989	-1.473974	1.151104	0.004924	0.712391
-26.751840	-1.362818	1.156109	0.005044	0.712384
-26.420471	-1.420048	1.161114	0.004982	0.712388
-26.049776	-1.484833	1.166118	0.004913	0.712391
-26.744294	-1.365379	1.171123	0.005042	0.712383
-26.523484	-1.406435	1.176128	0.005001	0.712380
-26.709898	-1.518382	1.181133	0.005035	0.712091
-27.324220	-1.409258	1.186138	0.005149	0.712091
-27.435678	-1.387192	1.191142	0.005170	0.712095
-27.572924	-1.369186	1.196147	0.005195	0.712083
-27.210325	-1.428771	1.201152	0.005127	0.712093
-27.371490	-1.403331	1.206157	0.005157	0.712087
-27.352402	-1.406564	1.211162	0.005153	0.712088
-27.433857	-1.512329	1.216166	0.005168	0.711849
-28.551872	-1.361053	1.221171	0.005376	0.711754
-28.177050	-1.422155	1.226176	0.005306	0.711765
-27.954803	-1.465738	1.231181	0.005265	0.711758
-28.499297	-1.369485	1.236186	0.005366	0.711757
-28.111630	-1.434793	1.241190	0.005293	0.711765
-28.214556	-1.422273	1.246195	0.005312	0.711754
-28.402545	-1.481055	1.251200	0.005347	0.711570
-29.612033	-1.325428	1.256205	0.005572	0.711451
-29.219116	-1.395471	1.261210	0.005499	0.711451
-28.547497	-1.512438	1.266214	0.005373	0.711457
-29.349626	-1.375047	1.271219	0.005522	0.711447
-29.343171	-1.371060	1.276224	0.005521	0.711457
-28.981950	-1.439484	1.281229	0.005453	0.711450
-29.154427	-1.452832	1.286234	0.005485	0.711362
-29.900766	-1.431618	1.291238	0.005624	0.711140
-29.645425	-1.482309	1.296243	0.005576	0.711130
-29.681304	-1.472383	1.301248	0.005583	0.711137
-29.749489	-1.463584	1.306253	0.005595	0.711131
-30.135210	-1.394955	1.311258	0.005667	0.711131
-30.109824	-1.396299	1.316262	0.005662	0.711138
-30.178265	-1.442280	1.321267	0.005674	0.711022
-30.769867	-1.413517	1.326272	0.005784	0.710870
-30.459507	-1.472408	1.331277	0.005726	0.710863
-30.890604	-1.395183	1.336282	0.005806	0.710864
-30.898231	-1.391153	1.341286	0.005807	0.710870
-30.618857	-1.447416	1.346291	0.005755	0.710858
-30.456876	-1.473103	1.351296	0.005725	0.710864
-30.975591	-1.493813	1.356301	0.005821	0.710639
-32.158780	-1.338987	1.361306	0.006041	0.710527
-31.326998	-1.484938	1.366310	0.005886	0.710532
-31.486665	-1.460771	1.371315	0.005916	0.710524
-31.848379	-1.393017	1.376320	0.005983	0.710531
-31.495199	-1.458132	1.381325	0.005917	0.710527
-31.583332	-1.443040	1.386330	0.005933	0.710527
-32.099944	-1.464105	1.391334	0.006029	0.710301
-33.101013	-1.331352	1.396339	0.006215	0.710210
-32.456772	-1.440800	1.401344	0.006095	0.710221
-32.300751	-1.472069	1.406349	0.006066	0.710215
-32.978391	-1.352662	1.411354	0.006192	0.710213
-32.588395	-1.418246	1.416358	0.006119	0.710221
-32.770595	-1.393224	1.421363	0.006152	0.710207
-32.735335	-1.441674	1.426368	0.006146	0.710123
-33.533215	-1.416056	1.431373	0.006294	0.709890
-33.352264	-1.449932	1.436378	0.006260	0.709887
-34.011102	-1.330047	1.441382	0.006382	0.709893
-33.908727	-1.354448	1.446387	0.006363	0.709881
-33.250318	-1.464904	1.451392	0.006240	0.709895
-33.551155	-1.413621	1.456397	0.006296	0.709891
-33.911355	-1.349768	1.461402	0.006363	0.709891
-33.658176	-1.499599	1.466406	0.006316	0.709682
-34.412042	-1.413390	1.471411	0.006456	0.709586
-34.551725	-1.383099	1.476416	0.006481	0.709597
-34.258279	-1.438312	1.481421	0.006427	0.709592
-34.513828	-1.395566	1.486426	0.006474	0.709587
-34.369445	-1.416760	1.491430	0.006447	0.709596
-34.649239	-1.370982	1.496435	0.006499	0.709588
-34.684172	-1.480498	1.501440	0.006505	0.709357
-35.179083	-1.439517	1.506445	0.006597	0.709263
-35.604827	-1.365735	1.511450	0.006676	0.709259
-35.445437	-1.392180	1.516454	0.006646	0.709264
-35.316681	-1.419172	1.521459	0.006622	0.709256
-35.392661	-1.400510	1.526464	0.006636	0.709267
-35.474237	-1.389626	1.531469	0.006651	0.709260
-35.459525	-1.471050	1.536474	0.006648	0.709103
-36.090176	-1.431938	1.541478	0.006765	0.708956
-36.179274	-1.420921	1.546483	0.006781	0.708947
-36.180067	-1.417688	1.551488	0.006781	0.708954
-36.042846	-1.442640	1.556493	0.006755	0.708953
-36.380282	-1.382801	1.561498	0.006818	0.708953
-36.188123	-1.415478	1.566502	0.006782	0.708957
-36.178260	-1.505668	1.571507	0.006780	0.708780
-37.268383	-1.381550	1.576512	0.006983	0.708640
-37.286506	-1.380958	1.581517	0.006986	0.708635
-37.168350	-1.402552	1.586522	0.006964	0.708634
-36.637565	-1.494766	1.591526	0.006865	0.708640
-37.541470	-1.337938	1.596531	0.007033	0.708632
-37.564594	-1.329091	1.601536	0.007037	0.708642
-37.007783	-1.458945	1.606541	0.006933	0.708581
-37.795844	-1.438342	1.611546	0.007079	0.708341
-37.732596	-1.446060	1.616550	0.007067	0.708349
-37.917024	-1.416099	1.621555	0.007101	0.708343
-37.861071	-1.425165	1.626560	0.007091	0.708345
-37.882336	-1.422260	1.631565	0.007094	0.708344
-37.946032	-1.413934	1.636570	0.007106	0.708338
-37.809702	-1.520276	1.641574	0.007081	0.708174
-39.242754	-1.350575	1.646579	0.007347	0.708003
-38.577445	-1.465060	1.651584	0.007223	0.708012
-38.398223	-1.498161	1.656589	0.007189	0.708010
-39.087421	-1.378229	1.661594	0.007317	0.708004
-38.983684	-1.393204	1.666598	0.007298	0.708012
-39.071287	-1.383847	1.671603	0.007314	0.708000
-38.929524	-1.476054	1.676608	0.007287	0.707866
-40.132331	-1.346024	1.681613	0.007511	0.707697
-39.624674	-1.438834	1.686618	0.007416	0.707693
-39.413977	-1.472020	1.691622	0.007377	0.707702
-40.102178	-1.355530	1.696627	0.007505	0.707690
-40.039316	-1.363222	1.701632	0.007493	0.707698
-39.524345	-1.458347	1.706637	0.007397	0.707692
-39.612866	-1.480455	1.711642	0.007413	0.707616
-40.579138	-1.427946	1.716646	0.007593	0.707376
-40.514667	-1.444483	1.721651	0.007580	0.707367
-40.721011	-1.405748	1.726656	0.007619	0.707371
-40.788643	-1.394771	1.731661	0.007631	0.707369
-40.770757	-1.398882	1.736666	0.007627	0.707368
-40.630046	-1.419830	1.741670	0.007601	0.707377
-40.571438	-1.450062	1.746675	0.007590	0.707337
-41.285354	-1.448274	1.751680	0.007723	0.707086
-41.195103	-1.466839	1.756685	0.007705	0.707081
-41.908916	-1.340097	1.761690	0.007838	0.707081
-41.798340	-1.357192	1.766694	0.007817	0.707087
-41.548998	-1.407030	1.771699	0.007771	0.707076
-41.531373	-1.405924	1.776704	0.007767	0.707085
-41.622962	-1.390404	1.781709	0.007784	0.707084
-42.078561	-1.461076	1.786714	0.007869	0.706779
-42.168070	-1.458283	1.791718	0.007885	0.706753
-42.481104	-1.407252	1.796723	0.007943	0.706744
-42.677403	-1.369959	1.801728	0.007979	0.706749
-42.381541	-1.424124	1.806733	0.007924	0.706747
-42.139876	-1.468202	1.811738	0.007879	0.706745
-42.319950	-1.435004	1.816742	0.007912	0.706748
-43.469642	-1.384785	1.821747	0.008126	0.706438
-43.147560	-1.438538	1.826752	0.008066	0.706446
-43.376210	-1.399361	1.831757	0.008108	0.706443
-43.558512	-1.368990	1.836762	0.008142	0.706439
-43.352681	-1.401399	1.841766	0.008103	0.706448
-43.295793	-1.417394	1.846771	0.008092	0.706437
-43.385767	-1.397578	1.851776	0.008109	0.706445
-43.475599	-1.468659	1.856781	0.008125	0.706270
-44.666558	-1.328329	1.861786	0.008347	0.706126
-44.267034	-1.397015	1.866790	0.008272	0.706131
-44.205176	-1.412613	1.871795	0.008261	0.706123
-44.054644	-1.435477	1.876800	0.008232	0.706131
-44.032599	-1.442269	1.881805	0.008228	0.706126
-44.816535	-1.304261	1.886810	0.008374	0.706123
-44.498804	-1.394041	1.891814	0.008314	0.706057
-44.945278	-1.413525	1.896819	0.008397	0.705858
-44.965476	-1.407586	1.901824	0.008401	0.705863
-44.994307	-1.404687	1.906829	0.008406	0.705859
-44.963128	-1.412563	1.911834	0.008400	0.705855
-44.898124	-1.419329	1.916838	0.008388	0.705865
-45.275298	-1.356235	1.921843	0.008457	0.705857
-45.174077	-1.458078	1.926848	0.008438	0.705689
-46.000118	-1.391768	1.931853	0.008592	0.705526
-46.109909	-1.374435	1.936858	0.008612	0.705522
-45.608549	-1.461902	1.941862	0.008519	0.705527
-46.039118	-1.387695	1.946867	0.008599	0.705522
-46.158609	-1.364677	1.951872	0.008621	0.705526
-45.908666	-1.409417	1.956877	0.008574	0.705526
-46.127494	-1.452963	1.961882	0.008614	0.705360
-46.860272	-1.395289	1.966886	0.008751	0.705214
-46.835322	-1.404922	1.971891	0.008746	0.705204
-46.580336	-1.447035	1.976896	0.008698	0.705211
-46.729934	-1.420705	1.981901	0.008726	0.705211
-47.052640	-1.365492	1.986906	0.008785	0.705207
-46.821803	-1.401749	1.991910	0.008742	0.705217
-46.586577	-1.541938	1.996915	0.008698	0.705019
-47.719030	-1.404889	2.001920	0.008909	0.704889

-47.583667	-1.430397	2.011917	0.008883	0.704887
-47.800305	-1.392609	2.021914	0.008923	0.704887
-47.504060	-1.445673	2.031910	0.008867	0.704887
-47.923545	-1.371295	2.041907	0.008945	0.704887
-47.801603	-1.393092	2.051904	0.008922	0.704888
-47.687360	-1.415649	2.061901	0.008900	0.704884
-48.010884	-1.358650	2.071898	0.008960	0.704884
-47.713526	-1.413193	2.081894	0.008904	0.704882
-47.750391	-1.405282	2.091891	0.008910	0.704885
-47.891447	-1.380774	2.101888	0.008936	0.704885
-47.641502	-1.426127	2.111885	0.008889	0.704884
-47.802945	-1.397635	2.121882	0.008919	0.704885
-47.539971	-1.373332	2.131878	0.008869	0.705029
-46.862094	-1.406133	2.141875	0.008743	0.705207
-46.917654	-1.394693	2.151872	0.008753	0.705211
-46.879869	-1.401719	2.161869	0.008745	0.705211
-46.985186	-1.384359	2.171866	0.008764	0.705209
-46.499734	-1.371804	2.181862	0.008673	0.705410
-46.038815	-1.396789	2.191859	0.008587	0.705526
-45.839750	-1.432799	2.201856	0.008550	0.705526
-45.934651	-1.417840	2.211853	0.008567	0.705522
-45.885835	-1.389548	2.221850	0.008557	0.705598
-44.821701	-1.451923	2.231846	0.008359	0.705855
-44.988848	-1.420900	2.241843	0.008389	0.705858
-44.885042	-1.438801	2.251840	0.008370	0.705860
-44.779635	-1.458114	2.261837	0.008349	0.705860
-44.585578	-1.365489	2.271834	0.008313	0.706117
-44.046383	-1.459875	2.281830	0.008212	0.706121
-44.221665	-1.428141	2.291827	0.008244	0.706123
-44.213236	-1.374344	2.301824	0.008242	0.706235
-43.530320	-1.394808	2.311821	0.008114	0.706440
-43.341129	-1.429716	2.321818	0.008079	0.706438
-43.558933	-1.391180	2.331814	0.008119	0.706438
-42.730735	-1.388219	2.341811	0.007964	0.706742
-42.496451	-1.426924	2.351808	0.007920	0.706749
-42.478722	-1.432474	2.361805	0.007916	0.706745
-42.310842	-1.391172	2.371802	0.007885	0.706889
-41.481055	-1.446819	2.381798	0.007730	0.707075
-41.549346	-1.434858	2.391795	0.007742	0.707076
-41.378195	-1.465382	2.401792	0.007710	0.707076
-41.201492	-1.391002	2.411789	0.007676	0.707290
-40.963832	-1.393662	2.421786	0.007631	0.707370
-40.835902	-1.417416	2.431782	0.007607	0.707369
-40.617428	-1.399280	2.441779	0.007566	0.707485
-39.578925	-1.480704	2.451776	0.007372	0.707694
-39.674639	-1.463115	2.461773	0.007390	0.707696
-39.986152	-1.409789	2.471770	0.007447	0.707692
-39.309085	-1.422079	2.481766	0.007321	0.707911
-39.226831	-1.389634	2.491763	0.007305	0.708006
-38.792365	-1.464945	2.501760	0.007223	0.708011
-38.914492	-1.411268	2.511757	0.007246	0.708076
-38.009016	-1.441507	2.521754	0.007077	0.708340
-38.075341	-1.430091	2.531750	0.007089	0.708340
-38.229828	-1.402105	2.541747	0.007117	0.708342
-37.649520	-1.405934	2.551744	0.007008	0.708542
-37.201740	-1.439333	2.561741	0.006924	0.708636
-37.308298	-1.422425	2.571738	0.006944	0.708633
-37.137049	-1.425572	2.581734	0.006912	0.708688
-36.527000	-1.402486	2.591731	0.006797	0.708953
-36.118207	-1.475359	2.601728	0.006721	0.708954
-36.548462	-1.399746	2.611725	0.006800	0.708953
-35.869293	-1.402319	2.621722	0.006674	0.709191
-35.738850	-1.391726	2.631718	0.006649	0.709259
-35.404197	-1.452712	2.641715	0.006586	0.709258
-35.370045	-1.400896	2.651712	0.006579	0.709374
-34.485129	-1.449670	2.661709	0.006414	0.709593
-34.745156	-1.404946	2.671706	0.006462	0.709591
-34.668216	-1.419728	2.681702	0.006447	0.709590
-34.113211	-1.391886	2.691699	0.006343	0.709844
-33.670063	-1.447151	2.701696	0.006260	0.709892
-33.870472	-1.413483	2.711693	0.006297	0.709889
-33.689790	-1.378070	2.721690	0.006263	0.710025
-32.917065	-1.422186	2.731686	0.006119	0.710213
-32.895112	-1.426034	2.741683	0.006114	0.710214
-32.913232	-1.421490	2.751680	0.006117	0.710218
-32.171844	-1.402798	2.761677	0.005979	0.710520
-32.076674	-1.415312	2.771674	0.005960	0.710530
-32.026940	-1.424190	2.781670	0.005951	0.710530
-31.803684	-1.400093	2.791667	0.005909	0.710659
-30.854770	-1.465296	2.801664	0.005732	0.710867
-31.249860	-1.394708	2.811661	0.005805	0.710868
-31.202720	-1.403710	2.821658	0.005795	0.710868
-30.733262	-1.362529	2.831654	0.005707	0.711118
-30.315938	-1.428608	2.841651	0.005629	0.711136
-30.611175	-1.376990	2.851648	0.005684	0.711135
-29.901768	-1.391797	2.861645	0.005551	0.711358
-29.536073	-1.410436	2.871642	0.005483	0.711452
-29.493713	-1.419604	2.881638	0.005474	0.711450
-29.451171	-1.386256	2.891635	0.005466	0.711532
-28.680890	-1.411291	2.901632	0.005322	0.711757
-28.683818	-1.411528	2.911629	0.005322	0.711756
-28.651512	-1.418435	2.921626	0.005316	0.711755
-28.028510	-1.386368	2.931622	0.005199	0.712041
-27.814098	-1.402275	2.941619	0.005159	0.712086
-27.839854	-1.396797	2.951616	0.005163	0.712089
-27.511185	-1.391332	2.961613	0.005101	0.712217
-26.909616	-1.413491	2.971610	0.004989	0.712388
-27.198243	-1.364038	2.981606	0.005042	0.712385
-26.786345	-1.428970	2.991603	0.004965	0.712402
-26.177670	-1.383768	3.001600	0.004851	0.712709
-25.926701	-1.428616	3.011597	0.004804	0.712710
-25.992991	-1.419094	3.021594	0.004816	0.712706
-25.820865	-1.378844	3.031590	0.004783	0.712848
-24.961379	-1.446521	3.041587	0.004623	0.713019
-25.226452	-1.398990	3.051584	0.004672	0.713021
-25.040551	-1.430634	3.061581	0.004637	0.713024
-24.319179	-1.399826	3.071578	0.004502	0.713342
-24.211481	-1.412231	3.081574	0.004482	0.713357
-23.916021	-1.467243	3.091571	0.004426	0.713353
-24.346445	-1.341414	3.101568	0.004506	0.713452
-23.152807	-1.454277	3.111565	0.004283	0.713651
-23.458511	-1.401630	3.121562	0.004339	0.713648
-23.402885	-1.411396	3.131558	0.004329	0.713649
-22.761301	-1.387180	3.141555	0.004209	0.713926
-22.639774	-1.386273	3.151552	0.004186	0.713971
-22.433907	-1.423789	3.161549	0.004147	0.713971
-22.377682	-1.369558	3.171546	0.004136	0.714099
-21.463205	-1.444146	3.181542	0.003965	0.714276
-21.281877	-1.476542	3.191539	0.003931	0.714276
-21.712855	-1.399181	3.201536	0.004011	0.714278
-20.726871	-1.445555	3.211533	0.003827	0.714536
-20.991974	-1.361223	3.221530	0.003876	0.714610
-20.527553	-1.444957	3.231526	0.003789	0.714609
-20.794226	-1.354161	3.241523	0.003838	0.714696
-19.721661	-1.438637	3.251520	0.003638	0.714909
-19.871804	-1.412018	3.261517	0.003665	0.714909
-19.941187	-1.400929	3.271514	0.003678	0.714908
-19.213579	-1.397640	3.281510	0.003542	0.715172
-18.877929	-1.429162	3.291507	0.003479	0.715229
-18.880053	-1.427810	3.301504	0.003479	0.715232
-18.758575	-1.414870	3.311501	0.003455	0.715302
-18.221580	-1.388383	3.321498	0.003355	0.715545
-17.803848	-1.465490	3.331494	0.003277	0.715540
-18.100297	-1.411548	3.341491	0.003332	0.715543
-17.375250	-1.446705	3.351488	0.003196	0.715731
-16.923511	-1.450262	3.361485	0.003112	0.715884
-17.041299	-1.431420	3.371482	0.003133	0.715881
-16.967188	-1.447512	3.381478	0.003119	0.715876
-16.436106	-1.437062	3.391475	0.003019	0.716085
-16.312731	-1.436842	3.401472	0.002996	0.716130
-16.204437	-1.455315	3.411469	0.002975	0.716132
-16.278547	-1.379080	3.421466	0.002989	0.716258
-15.226001	-1.474523	3.431462	0.002792	0.716441
-15.507248	-1.422974	3.441459	0.002844	0.716445
-15.344102	-1.451730	3.451456	0.002813	0.716446
-14.885897	-1.378698	3.461453	0.002727	0.716753
-14.202142	-1.500070	3.471450	0.002600	0.716755
-14.358532	-1.474276	3.481446	0.002628	0.716752
-14.357658	-1.403363	3.491443	0.002628	0.716893
-13.222504	-1.510581	3.501440	0.002416	0.717082
-13.468062	-1.465785	3.511437	0.002461	0.717085
-13.629197	-1.438989	3.521434	0.002491	0.717082
-12.860954	-1.454585	3.531430	0.002347	0.717323
-12.584489	-1.477756	3.541427	0.002295	0.717375
-12.459231	-1.499247	3.551424	0.002271	0.717378
-12.707294	-1.436378	3.561421	0.002317	0.717416
-11.594628	-1.491394	3.571418	0.002110	0.717700
-11.748011	-1.465586	3.581414	0.002138	0.717698
-11.542228	-1.501893	3.591411	0.002099	0.717699
-11.468827	-1.448941	3.601408	0.002085	0.717830
-10.648652	-1.502325	3.611405	0.001932	0.718015
-10.798003	-1.477157	3.621402	0.001959	0.718013
-10.744316	-1.488272	3.631398	0.001948	0.718010
-10.171305	-1.461163	3.641395	0.001841	0.718266
-9.680895	-1.506254	3.651392	0.001749	0.718351
-9.627567	-1.516909	3.661389	0.001739	0.718349
-9.691349	-1.505479	3.671386	0.001751	0.718350
-9.110820	-1.471051	3.681382	0.001642	0.718623
-8.821751	-1.515655	3.691379	0.001588	0.718638
-8.788637	-1.520453	3.701376	0.001581	0.718641
-8.812312	-1.468691	3.711373	0.001585	0.718736
-7.768069	-1.543588	3.721370	0.001390	0.718956
-7.900676	-1.518712	3.731366	0.001414	0.718959
-7.771799	-1.543377	3.741363	0.001390	0.718956
-7.716605	-1.465584	3.751360	0.001379	0.719130
-7.077156	-1.509538	3.761357	0.001260	0.719269
-7.154873	-1.496537	3.771354	0.001274	0.719268
-7.184442	-1.480183	3.781350	0.001279	0.719291
-6.254883	-1.490868	3.791347	0.001105	0.719597
-5.990340	-1.537911	3.801344	0.001055	0.719598
-6.329556	-1.477586	3.811341	0.001118	0.719599
-5.773862	-1.506136	3.821338	0.001014	0.719739
-5.219949	-1.526459	3.831334	0.000911	0.719894
-5.029590	-1.559812	3.841331	0.000875	0.719896
-5.109861	-1.545922	3.851328	0.000889	0.719896
-4.559912	-1.547665	3.861325	0.000786	0.720086
-4.290209	-1.528285	3.871322	0.000736	0.720220
-4.245771	-1.537635	3.881318	0.000727	0.720218
-4.089046	-1.565236	3.891315	0.000697	0.720219
-3.448006	-1.545320	3.901312	0.000577	0.720484
-3.368549	-1.532044	3.911309	0.000562	0.720539
-3.068663	-1.586091	3.921306	0.000506	0.720539
-3.388168	-1.517925	3.931302	0.000565	0.720562
-2.438775	-1.528621	3.941299	0.000388	0.720874
-2.410219	-1.533753	3.951296	0.000382	0.720875
-2.309668	-1.551150	3.961293	0.000363	0.720877
-2.464455	-1.464283	3.971290	0.000391	0.720994
-1.809714	-1.521204	3.981286	0.000269	0.721113
-1.924730	-1.498504	3.991283	0.000289	0.721118
-1.810406	-1.464705	4.001280	0.000268	0.721225
-1.347075	-1.440731	4.011277	0.000181	0.721435
-1.500764	-1.414285	4.021274	0.000209	0.721435
-1.333953	-1.365711	4.031270	0.000178	0.721589
-1.238532	-1.306833	4.041267	0.000159	0.721739
-0.950134	-1.352784	4.051264	0.000105	0.721751
-0.980813	-1.183032	4.061261	0.000110	0.722074
-0.819128	-1.214136	4.071258	0.000080	0.722071
-0.614462	-1.134976	4.081254	0.000041	0.722299
-0.630955	-1.098332	4.091251	0.000044	0.722366
-0.687274	-0.974207	4.101248	0.000054	0.722590
-0.652164	-0.929015	4.111245	0.000047	0.722692
-0.646695	-0.792694	4.121242	0.000045	0.722963
-0.564304	-0.752825	4.131238	0.000029	0.723070
-0.579320	-0.614977	4.141235	0.000031	0.723336
-0.364536	-0.557108	4.151232	-0.000009	0.723526
-0.361060	-0.481890	4.161229	-0.000010	0.723675
-0.316134	-0.350132	4.171226	-0.000019	0.723950
-0.284213	-0.238992	4.181222	-0.000026	0.724179
-0.247242	-0.137495	4.191219	-0.000033	0.724392
-0.243772	-0.013471	4.201216	-0.000034	0.724637
-0.179586	0.102743	4.211213	-0.000047	0.724887
0.000000	0.238992	4.221210	-0.000081	0.725217

-0.116679	0.882629	4.226214	-0.000060	0.726435
-0.016256	2.128007	4.231219	-0.000079	0.728897
0.407806	3.924900	4.236224	-0.000160	0.732531
0.824314	6.272026	4.241229	-0.000239	0.737204
0.766144	9.213210	4.246234	-0.000230	0.742821
1.271529	12.542678	4.251238	-0.000327	0.749321
1.713851	16.324354	4.256243	-0.000412	0.756592
2.022318	20.546933	4.261248	-0.000472	0.764567
2.246247	25.184884	4.266253	-0.000517	0.773195
2.951119	30.097683	4.271258	-0.000652	0.782380
3.357106	35.425317	4.276262	-0.000731	0.792107
3.630677	41.074763	4.281267	-0.000786	0.802243
4.011864	47.019005	4.286272	-0.000861	0.812800
4.520613	53.216281	4.291277	-0.000960	0.823696
5.110673	59.683514	4.296282	-0.001075	0.834932
5.592508	66.384522	4.301286	-0.001169	0.846379
5.931866	73.328120	4.306291	-0.001237	0.858032
6.588224	80.428859	4.311296	-0.001364	0.869875
7.589596	87.664826	4.316301	-0.001555	0.881875
8.230660	95.133487	4.321306	-0.001680	0.893981
8.958040	102.756660	4.326310	-0.001820	0.906191
9.172010	110.594488	4.331315	-0.001866	0.918430
10.125671	118.414517	4.336320	-0.002048	0.930679
10.891900	126.393209	4.341325	-0.002197	0.942957
11.575725	134.496678	4.346330	-0.002329	0.955241
12.160760	142.697046	4.351334	-0.002444	0.967485
12.914651	150.958166	4.356339	-0.002590	0.979706
13.474963	159.353642	4.361344	-0.002700	0.991920
14.018508	167.774477	4.366349	-0.002807	1.004017
14.492113	176.250615	4.371354	-0.002901	1.016029
14.899504	184.782287	4.376358	-0.002982	1.027962
15.785492	193.254178	4.381363	-0.003153	1.039789
16.602707	201.786717	4.386368	-0.003311	1.051548
17.129667	210.389422	4.391373	-0.003415	1.063204
17.661419	219.021915	4.396378	-0.003520	1.074773
18.687298	227.567248	4.401382	-0.003717	1.086216
19.353019	236.192017	4.406387	-0.003847	1.097561
19.996403	244.835292	4.411392	-0.003972	1.108809
20.502772	253.500561	4.416397	-0.004072	1.119942
21.212102	262.122129	4.421402	-0.004210	1.130953
21.749868	270.775459	4.426406	-0.004316	1.141861
22.308351	279.442145	4.431411	-0.004426	1.152687
23.022410	288.043876	4.436416	-0.004565	1.163364
23.795133	296.628868	4.441421	-0.004715	1.173936
24.592482	305.193362	4.446426	-0.004869	1.184394
24.966194	313.846874	4.451430	-0.004945	1.194779
25.342838	322.451526	4.456435	-0.005020	1.205018
25.788805	331.057506	4.461440	-0.005109	1.215186
26.302163	339.626877	4.466445	-0.005211	1.225240
27.018112	348.167743	4.471450	-0.005350	1.235219
27.555444	356.704026	4.476454	-0.005456	1.245078
27.792483	365.275941	4.481459	-0.005506	1.254842
28.200895	373.799446	4.486464	-0.005588	1.264509
28.965240	382.267693	4.491469	-0.005736	1.274107
29.501496	390.737975	4.496474	-0.005841	1.283593
30.166127	399.205451	4.501478	-0.005971	1.293030
30.606301	407.682106	4.506483	-0.006058	1.302367
31.122173	416.227715	4.511488	-0.006160	1.311726
31.668476	424.697902	4.516493	-0.006268	1.320943
31.899585	433.148084	4.521498	-0.006317	1.330018
32.685055	441.518561	4.526502	-0.006468	1.339045
32.925660	449.950283	4.531507	-0.006519	1.347980
33.210765	458.384172	4.536512	-0.006578	1.356866
33.615524	466.755580	4.541517	-0.006659	1.365650
33.875056	475.163244	4.546522	-0.006713	1.374390
34.319569	483.528516	4.551526	-0.006801	1.383063
34.699196	491.892832	4.556531	-0.006878	1.391670
35.203227	500.224791	4.561536	-0.006977	1.400212
35.538449	508.569217	4.566541	-0.007045	1.408686
35.828834	516.919590	4.571546	-0.007105	1.417108
36.404559	525.216311	4.576550	-0.007218	1.425474
36.782500	533.550446	4.581555	-0.007294	1.433795
37.129773	541.861932	4.586560	-0.007364	1.442041
37.535549	550.170226	4.591565	-0.007445	1.450246
38.076701	558.455107	4.596570	-0.007552	1.458403
38.549427	566.747366	4.601574	-0.007645	1.466512
38.850355	575.104664	4.606579	-0.007707	1.474611
39.395309	583.358800	4.611584	-0.007814	1.482605
39.809672	591.634806	4.616589	-0.007897	1.490556
40.263230	599.896546	4.621594	-0.007987	1.498458
40.518931	608.188039	4.626598	-0.008040	1.506316
40.728967	616.488464	4.631603	-0.008085	1.514134
41.308967	624.692074	4.636608	-0.008199	1.521878
41.985163	632.906439	4.641613	-0.008330	1.529607
42.450956	641.156602	4.646618	-0.008423	1.537299
42.741921	649.429413	4.651622	-0.008482	1.544946
43.087490	657.699892	4.656627	-0.008552	1.552562
43.442666	665.937360	4.661632	-0.008624	1.560112
43.839084	674.163814	4.666637	-0.008703	1.567621
44.164458	682.408910	4.671642	-0.008770	1.575101
44.936365	690.582600	4.676646	-0.008919	1.582546
45.251684	698.825273	4.681651	-0.008983	1.589952
45.695718	707.051605	4.686656	-0.009072	1.597328
46.422774	715.213599	4.691661	-0.009212	1.604652
46.736866	723.459939	4.696666	-0.009277	1.611959
47.220690	731.668915	4.701670	-0.009372	1.619224
47.628642	739.873902	4.706675	-0.009454	1.626442
48.076260	748.136880	4.711680	-0.009543	1.633684
48.447052	756.331608	4.716685	-0.009617	1.640824
49.057497	764.475797	4.721690	-0.009737	1.647923
49.690367	772.658452	4.726694	-0.009860	1.655027
50.171157	780.830655	4.731699	-0.009955	1.662071
50.416291	789.060986	4.736704	-0.010006	1.669102
50.815548	797.264205	4.741709	-0.010086	1.676102
51.263119	805.433317	4.746714	-0.010175	1.683050
51.509524	813.646740	4.751718	-0.010227	1.689980
52.080313	821.808325	4.756723	-0.010338	1.696881
52.502527	829.976519	4.761728	-0.010423	1.703740
53.054003	838.152270	4.766733	-0.010531	1.710594
53.038304	846.403194	4.771738	-0.010533	1.717410
53.468981	854.548513	4.776742	-0.010619	1.724169
53.920305	862.693460	4.781747	-0.010709	1.730904
54.560684	870.830063	4.786752	-0.010834	1.737630
55.106901	878.972287	4.791757	-0.010941	1.744322
55.591394	887.139037	4.796762	-0.011037	1.751001
55.856349	895.339819	4.801766	-0.011091	1.757654
55.894991	903.529295	4.806771	-0.011104	1.764244
56.446225	911.663934	4.811776	-0.011212	1.770830
57.227000	919.782348	4.816781	-0.011363	1.777407
57.695925	927.928181	4.821786	-0.011456	1.783943
58.287739	936.098725	4.826790	-0.011572	1.790489
58.830996	944.268677	4.831795	-0.011679	1.797005
59.267509	952.408422	4.836800	-0.011765	1.803460
59.725762	960.545887	4.841805	-0.011856	1.809893
60.150288	968.685943	4.846810	-0.011941	1.816301
60.633208	976.811811	4.851814	-0.012036	1.822683
60.892669	984.978883	4.856819	-0.012090	1.829047
61.421629	993.122491	4.861824	-0.012194	1.835403
61.909572	1001.244706	4.866829	-0.012291	1.841715
61.965712	1009.427094	4.871834	-0.012307	1.848001
62.501008	1017.560726	4.876838	-0.012412	1.854285
62.988669	1025.664322	4.881843	-0.012508	1.860519
63.516557	1033.790451	4.886848	-0.012612	1.866753
63.986932	1041.952624	4.891853	-0.012705	1.872988
64.290906	1050.085351	4.896858	-0.012767	1.879160
65.007470	1058.162134	4.901862	-0.012906	1.885317
65.272074	1066.325122	4.906867	-0.012961	1.891467
65.567766	1074.466281	4.911872	-0.013022	1.897584
66.022683	1082.585501	4.916877	-0.013112	1.903683
66.379868	1090.708297	4.921882	-0.013184	1.909754
66.944581	1098.826100	4.926886	-0.013295	1.915825
67.340230	1106.930656	4.931891	-0.013374	1.921849
67.571899	1115.081284	4.936896	-0.013422	1.927869
68.101362	1123.206775	4.941901	-0.013527	1.933884
68.432620	1131.315573	4.946906	-0.013594	1.939847
69.010163	1139.418626	4.951910	-0.013707	1.945814
69.324503	1147.593036	4.956915	-0.013771	1.951786
69.626959	1155.727198	4.961920	-0.013833	1.957709
70.301606	1163.787255	4.966925	-0.013964	1.963601
70.495332	1171.910126	4.971930	-0.014005	1.969469
70.905660	1180.038577	4.976934	-0.014087	1.975346
71.219314	1188.136103	4.981939	-0.014151	1.981174
71.791888	1196.217667	4.986944	-0.014263	1.987000
72.076107	1204.364134	4.991949	-0.014322	1.992825
72.320950	1212.472872	4.996954	-0.014373	1.998602
73.043097	1220.522791	5.001958	-0.014513	2.004370
73.426906	1228.634436	5.006963	-0.014590	2.010130
73.919499	1236.730248	5.011968	-0.014687	2.015874
74.411402	1244.838305	5.016973	-0.014784	2.021609
74.894166	1252.924426	5.021978	-0.014880	2.027312
75.209097	1261.081552	5.026982	-0.014944	2.033031
75.648133	1269.179803	5.031987	-0.015031	2.038706
75.900721	1277.283966	5.036992	-0.015084	2.044350
76.178019	1285.397851	5.041997	-0.015141	2.049987
76.390138	1293.510988	5.047002	-0.015186	2.055602
76.864479	1301.593574	5.052006	-0.015280	2.061207
77.149041	1309.695971	5.057011	-0.015338	2.066791
77.314346	1317.840445	5.062016	-0.015374	2.072377
77.690527	1325.919466	5.067021	-0.015450	2.077925
77.695628	1334.043607	5.072026	-0.015456	2.083451
78.029495	1342.134870	5.077030	-0.015524	2.088972
78.464168	1350.214706	5.082035	-0.015611	2.094482
78.787935	1358.296808	5.087040	-0.015676	2.099967
79.164821	1366.374739	5.092045	-0.015752	2.105440
79.513328	1374.495798	5.097050	-0.015822	2.110926
79.894664	1382.621388	5.102054	-0.015899	2.116403
80.077987	1390.694603	5.107059	-0.015939	2.121812
80.385693	1398.767850	5.112064	-0.016001	2.127219
80.735638	1406.865226	5.117069	-0.016072	2.132632
81.113746	1414.921396	5.122074	-0.016148	2.138007
81.480318	1423.013982	5.127078	-0.016222	2.143391
81.697137	1431.118551	5.132083	-0.016268	2.148755
81.879113	1439.239742	5.137088	-0.016307	2.154114
82.246904	1447.296410	5.142093	-0.016381	2.159434
82.542980	1455.354090	5.147098	-0.016442	2.164735
82.947336	1463.455839	5.152102	-0.016522	2.170062
83.417515	1471.528135	5.157107	-0.016615	2.175363
83.598674	1479.622557	5.162112	-0.016655	2.180638
83.910095	1487.704751	5.167117	-0.016718	2.185905
84.223746	1495.808542	5.172122	-0.016782	2.191173
84.457078	1503.922118	5.177126	-0.016831	2.196427
84.811983	1511.949481	5.182131	-0.016903	2.201625
85.229839	1520.000599	5.187136	-0.016986	2.206831
85.673460	1528.094996	5.192141	-0.017074	2.212054
85.565893	1536.215931	5.197146	-0.017059	2.217233
85.824564	1544.292339	5.202150	-0.017113	2.222404
86.202592	1552.339806	5.207155	-0.017189	2.227555
86.614047	1560.426879	5.212160	-0.017271	2.232722
86.881604	1568.503739	5.217165	-0.017326	2.237858
87.249567	1576.558116	5.222170	-0.017400	2.242977
87.903813	1584.604636	5.227174	-0.017528	2.248104
88.137166	1592.704757	5.232179	-0.017577	2.253217
88.430807	1600.791897	5.237184	-0.017637	2.258314
88.714552	1608.882924	5.242189	-0.017695	2.263402
89.068440	1616.944597	5.247194	-0.017767	2.268466
89.613597	1625.084609	5.252198	-0.017874	2.273584
89.828701	1633.143928	5.257203	-0.017919	2.278612
90.202873	1641.175812	5.262208	-0.017994	2.283625
90.487836	1649.260902	5.267213	-0.018053	2.288653
90.871981	1657.317676	5.272218	-0.018130	2.293660
90.972618	1665.420159	5.277222	-0.018154	2.298661
91.240322	1673.473962	5.282227	-0.018209	2.303635
91.503463	1681.541918	5.287232	-0.018264	2.308606
91.925122	1689.623627	5.292237	-0.018348	2.313588
92.256652	1697.662209	5.297242	-0.018415	2.318526
92.563803	1705.731239	5.302246	-0.018478	2.323469
92.807084	1713.803516	5.307251	-0.018529	2.328399
93.183061	1721.879134	5.312256	-0.018604	2.333331
93.509459	1729.958206	5.317261	-0.018670	2.338251
93.887975	1737.989531	5.322266	-0.018746	2.343135
94.415165	1746.051159	5.327270	-0.018850	2.348040
94.781550	1754.165280	5.332275	-0.018924	2.352953
95.046913	1762.227267	5.337280	-0.018979	2.357816
95.463057	1770.278963	5.342285	-0.019062	2.362675
95.863977	1778.322142	5.347290	-0.019142	2.367518
96.227415	1786.415652	5.352294	-0.019215	2.372378
96.454414	1794.472985	5.357299	-0.019263	2.377195
96.666176	1802.542034	5.362304	-0.019308	2.382008
96.981709	1810.613390	5.367309	-0.019372	2.386821
96.993030	1818.721369	5.372314	-0.019379	2.391622
97.245060	1826.801338	5.377318	-0.019432	2.396416
97.403404	1834.850004	5.382323	-0.019467	2.401174
97.611440	1842.890872	5.387328	-0.019511	2.405922
98.020719	1850.956127	5.392333	-0.019593	2.410691
97.908331	1859.063991	5.397338	-0.019577	2.415434
98.358661	1867.097885	5.402342	-0.019667	2.420169
98.706155	1875.137614	5.407347	-0.019737	2.424890
99.216028	1883.186259	5.412352	-0.019837	2.429619
99.440308	1891.350431	5.417357	-0.019885	2.434384
99.614884	1899.370400	5.422362	-0.019923	2.439053
99.956778	1907.417818	5.427366	-0.019992	2.443741
100.245736	1915.458152	5.432371	-0.020051	2.448411
100.489086	1923.512711	5.437376	-0.020102	2.453078
100.677221	1931.597606	5.442381	-0.020142	2.457749
101.008625	1939.614309	5.447386	-0.020209	2.462383
101.352920	1947.671609	5.452390	-0.020279	2.467032
101.657013	1955.742217	5.457395	-0.020341	2.471677
101.911458	1963.817459	5.462400	-0.020394	2.476312
102.284237	1971.856190	5.467405	-0.020469	2.480926
102.550938	1979.895104	5.472410	-0.020524	2.485524
102.915639	1987.949293	5.477414	-0.020597	2.490129
102.973572	1996.063309	5.482419	-0.020614	2.494737
103.569890	2004.062354	5.487424	-0.020730	2.499311
104.070585	2012.105917	5.492429	-0.020829	2.503895
104.260639	2020.185199	5.497434	-0.020870	2.508467
104.616361	2028.297426	5.502438	-0.020942	2.513062
104.859441	2036.339156	5.507443	-0.020992	2.517601
105.301852	2044.350775	5.512448	-0.021080	2.522129
105.404256	2052.423701	5.517453	-0.021105	2.526658
105.500991	2060.499339	5.522458	-0.021128	2.531181
105.831902	2068.581977	5.527462	-0.021195	2.535716
105.927175	2076.633914	5.532467	-0.021219	2.540209
106.239464	2084.662713	5.537472	-0.021282	2.544696
106.628858	2092.728167	5.542477	-0.021360	2.549202
106.734179	2100.798245	5.547482	-0.021385	2.553682
107.152753	2108.842586	5.552486	-0.021469	2.558161
107.370096	2116.879796	5.557491	-0.021515	2.562615
107.567218	2124.942188	5.562496	-0.021557	2.567074
107.801891	2133.020521	5.567501	-0.021606	2.571536
108.288572	2141.037216	5.572506	-0.021702	2.575974
108.626432	2149.091885	5.577510	-0.021770	2.580415
108.745586	2157.147298	5.582515	-0.021798	2.584833
109.076057	2165.187226	5.587520	-0.021865	2.589250
109.586868	2173.428134	5.592525	-0.021966	2.593781
109.770285	2181.427793	5.597530	-0.022005	2.598151
110.188001	2189.413815	5.602534	-0.022089	2.602521
110.456835	2197.429192	5.607539	-0.022144	2.606890
110.670037	2205.470583	5.612544	-0.022189	2.611262
110.794999	2213.546945	5.617549	-0.022218	2.615640
111.058214	2221.550931	5.622554	-0.022273	2.619981
111.478502	2229.569483	5.627558	-0.022356	2.624332
111.626494	2237.641357	5.632563	-0.022389	2.628687
111.899574	2245.701102	5.637568	-0.022446	2.633036
112.404644	2253.741102	5.642573	-0.022545	2.637383
112.773727	2261.759778	5.647578	-0.022619	2.641703
113.150618	2269.796981	5.652582	-0.022695	2.646025
113.534476	2277.845828	5.657587	-0.022772	2.650347
113.708530	2285.934324	5.662592	-0.022810	2.654670
114.115250	2293.978314	5.667597	-0.022891	2.658977
114.349993	2302.003061	5.672602	-0.022940	2.663255
114.775557	2310.048831	5.677606	-0.023025	2.667550
114.935619	2318.145437	5.682611	-0.023060	2.671848
114.965926	2326.233118	5.687616	-0.023071	2.676125
115.346286	2334.252251	5.692621	-0.023148	2.680383
115.373005	2342.260773	5.697626	-0.023158	2.684605
115.475255	2350.344057	5.702630	-0.023183	2.688864
115.805618	2358.392478	5.707635	-0.023250	2.693113
116.010282	2366.436786	5.712640	-0.023293	2.697346
116.086588	2374.511087	5.717645	-0.023313	2.701579
116.254936	2382.504585	5.722650	-0.023350	2.705769
116.916704	2390.531620	5.727654	-0.023478	2.710001
117.326114	2398.589214	5.732659	-0.023560	2.714226
117.496772	2406.641311	5.737664	-0.023597	2.718427
117.842533	2414.676661	5.742669	-0.023667	2.722624
117.885056	2422.739657	5.747674	-0.023681	2.726809
118.186392	2430.810235	5.752678	-0.023742	2.731008
118.347200	2438.873249	5.757683	-0.023778	2.735188
118.709016	2446.864974	5.762688	-0.023850	2.739338
118.984279	2454.929568	5.767693	-0.023907	2.743513
119.057642	2462.980094	5.772698	-0.023926	2.747662
119.477185	2471.069475	5.777702	-0.024010	2.751846
119.712485	2479.166936	5.782707	-0.024059	2.756016
120.084396	2487.144911	5.787712	-0.024134	2.760127
120.331302	2495.152722	5.792717	-0.024185	2.764240
120.587158	2503.170947	5.797722	-0.024238	2.768352
121.009435	2511.238734	5.802726	-0.024323	2.772493
121.312952	2519.273822	5.807731	-0.024385	2.776605
121.590740	2527.301886	5.812736	-0.024442	2.780705
121.955797	2535.318275	5.817741	-0.024515	2.784798
121.862508	2543.403621	5.822746	-0.024503	2.788893
122.393710	2551.443797	5.827750	-0.024608	2.792996
122.595942	2559.509481	5.832755	-0.024651	2.797086
122.868866	2567.516427	5.837760	-0.024707	2.801145
123.035980	2575.566568	5.842765	-0.024744	2.805214
123.335328	2583.587820	5.847770	-0.024805	2.809270
123.774931	2591.660640	5.852774	-0.024892	2.813354
123.915158	2599.716958	5.857779	-0.024924	2.817406
124.091094	2607.757808	5.862784	-0.024962	2.821447
124.075675	2615.829691	5.867789	-0.024965	2.825486
124.306853	2623.862454	5.872794	-0.025013	2.829515
124.722557	2631.929575	5.877798	-0.025096	2.833565
124.946432	2639.945690	5.882803	-0.025143	2.837573
124.909564	2647.981561	5.887808	-0.025142	2.841570
125.377862	2655.999710	5.892813	-0.025235	2.845582
125.693044	2664.017825	5.897818	-0.025299	2.849579
125.967867	2672.088505	5.902822	-0.025355	2.853594
126.315906	2680.098057	5.907827	-0.025426	2.857577
126.625823	2688.134658	5.912832	-0.025489	2.861566
127.082881	2696.171799	5.917837	-0.025579	2.865558
127.086155	2704.228248	5.922842	-0.025585	2.869529
127.424011	2712.295185	5.927846	-0.025654	2.873517
127.719932	2720.329901	5.932851	-0.025714	2.877482
127.551062	2728.385132	5.937856	-0.025688	2.881426
128.016589	2736.390142	5.942861	-0.025781	2.885375
128.248600	2744.424711	5.947866	-0.025829	2.889320
128.289862	2752.518436	5.952870	-0.025842	2.893278
128.608241	2760.543892	5.957875	-0.025907	2.897213
128.727379	2768.585191	5.962880	-0.025935	2.901138
129.167394	2776.596214	5.967885	-0.026022	2.905062
129.371288	2784.639864	5.972890	-0.026066	2.908982
129.688379	2792.763753	5.977894	-0.026130	2.912943
130.025557	2800.800001	5.982899	-0.026198	2.916857
130.066352	2808.799094	5.987904	-0.026212	2.920732
130.335737	2816.814166	5.992909	-0.026267	2.924621
130.514668	2824.841541	5.997914	-0.026306	2.928506
130.814622	2832.887850	6.002918	-0.026367	2.932402
130.834498	2840.969058	6.007923	-0.026376	2.936294
131.114170	2848.960642	6.012928	-0.026434	2.940152
131.439364	2856.977451	6.017933	-0.026500	2.944019
131.546373	2865.022116	6.022938	-0.026525	2.947884
131.670045	2873.096469	6.027942	-0.026554	2.951758
131.909362	2881.157914	6.032947	-0.026604	2.955626
132.142184	2889.136593	6.037952	-0.026653	2.959450
132.445587	2897.181639	6.042957	-0.026715	2.963304
132.426672	2905.215563	6.047962	-0.026717	2.967132
132.884264	2913.242252	6.052966	-0.026807	2.970975
132.945439	2921.320692	6.057971	-0.026824	2.974817
133.090719	2929.321653	6.062976	-0.026857	2.978622
133.440903	2937.339419	6.067981	-0.026927	2.982441
133.515648	2945.384431	6.072986	-0.026947	2.986254
133.907395	2953.406094	6.077990	-0.027025	2.990066
134.234713	2961.486059	6.082995	-0.027092	2.993898
134.333961	2969.513920	6.088000	-0.027116	2.997689
134.543078	2977.539733	6.093005	-0.027160	3.001480
134.953578	2985.529337	6.098010	-0.027242	3.005259
135.215898	2993.579394	6.103014	-0.027296	3.009054
135.179768	3001.666455	6.108019	-0.027295	3.012847
135.377027	3009.674559	6.113024	-0.027337	3.016609
135.871651	3017.701025	6.118029	-0.027435	3.020391
135.889093	3025.736880	6.123034	-0.027443	3.024148
135.915822	3033.809881	6.128038	-0.027454	3.027918
136.317668	3041.850571	6.133043	-0.027534	3.031687
136.477188	3049.885071	6.138048	-0.027569	3.035437
136.830589	3057.889341	6.143053	-0.027641	3.039177
136.863465	3065.901872	6.148058	-0.027652	3.042901
137.435438	3073.951360	6.153062	-0.027764	3.046663
137.618688	3081.998606	6.158067	-0.027804	3.050401
137.833071	3090.043172	6.163072	-0.027849	3.054135
137.998502	3098.080428	6.168077	-0.027885	3.057858
138.131274	3106.099799	6.173082	-0.027916	3.061567
138.475997	3114.113376	6.178086	-0.027985	3.065279
138.706014	3122.170950	6.183091	-0.028034	3.069001
139.057102	3130.252574	6.188096	-0.028104	3.072735
139.203290	3138.346029	6.193101	-0.028137	3.076460
139.310714	3146.305596	6.198106	-0.028163	3.080118
139.689820	3154.297582	6.203110	-0.028239	3.083799
139.832221	3162.353971	6.208115	-0.028271	3.087494
140.043778	3170.356404	6.213120	-0.028315	3.091163
140.303387	3178.417654	6.218125	-0.028369	3.094857
140.552353	3186.428112	6.223130	-0.028421	3.098522
140.779233	3194.476461	6.228134	-0.028469	3.102199
140.885523	3202.528031	6.233139	-0.028494	3.105868
141.337230	3210.492103	6.238144	-0.028584	3.109509
141.755004	3218.559269	6.243149	-0.028667	3.113190
141.779991	3226.609884	6.248154	-0.028677	3.116842
142.138483	3234.630599	6.253158	-0.028749	3.120491
142.294201	3242.654771	6.258163	-0.028784	3.124128
142.323471	3250.709197	6.263168	-0.028795	3.127769
142.671131	3258.767174	6.268173	-0.028865	3.131422
142.638355	3266.793964	6.273178	-0.028864	3.135039
142.759039	3274.842658	6.278182	-0.028892	3.138669
142.914957	3282.850743	6.283187	-0.028927	3.142277
143.210213	3290.854457	6.288192	-0.028987	3.145886
143.465243	3298.902780	6.293197	-0.029040	3.149509
143.525574	3306.997641	6.298202	-0.029057	3.153140
143.899160	3314.979934	6.303206	-0.029132	3.156730
144.101408	3323.003543	6.308211	-0.029175	3.160326
144.279215	3331.000309	6.313216	-0.029213	3.163906
144.645447	3339.043985	6.318221	-0.029287	3.167511
144.632874	3347.084573	6.323226	-0.029290	3.171094
144.956589	3355.131282	6.328230	-0.029356	3.174690
145.095874	3363.179751	6.333235	-0.029387	3.178274
145.439949	3371.183943	6.338240	-0.029457	3.181844
145.653286	3379.220404	6.343245	-0.029502	3.185418
145.609012	3387.265283	6.348250	-0.029499	3.188981
145.850493	3395.307378	6.353254	-0.029550	3.192551
146.085590	3403.339428	6.358259	-0.029599	3.196113
146.309566	3411.334231	6.363264	-0.029646	3.199653
146.477009	3419.376653	6.368269	-0.029683	3.203208
146.640556	3427.394443	6.373274	-0.029719	3.206748
146.962170	3435.412625	6.378278	-0.029784	3.210291
147.350969	3443.471857	6.383283	-0.029862	3.213851
147.511552	3451.498411	6.388288	-0.029897	3.217383
147.715283	3459.554738	6.393293	-0.029941	3.220926
147.892815	3467.529122	6.398298	-0.029979	3.224427
148.209066	3475.559945	6.403302	-0.030044	3.227956
148.284339	3483.667225	6.408307	-0.030063	3.231504
148.455062	3491.719500	6.413312	-0.030100	3.235028
148.658769	3499.708133	6.418317	-0.030144	3.238522
148.982960	3507.697189	6.423322	-0.030210	3.242017
149.301560	3515.704159	6.428326	-0.030274	3.245516
149.485920	3523.730181	6.433331	-0.030314	3.249014
149.674946	3531.777463	6.438336	-0.030355	3.252517
149.910069	3539.865993	6.443341	-0.030404	3.256037
149.866100	3547.849943	6.448346	-0.030401	3.259496
150.039093	3555.882357	6.453350	-0.030439	3.262981
150.346335	3563.927065	6.458355	-0.030502	3.266473
150.423214	3571.942274	6.463360	-0.030521	3.269939
150.894863	3580.009703	6.468365	-0.030615	3.273440
151.021224	3588.045648	6.473370	-0.030644	3.276910
150.976886	3596.052709	6.478374	-0.030641	3.280357
151.286616	3604.052851	6.483379	-0.030704	3.283811
151.533620	3612.047613	6.488384	-0.030755	3.287257
151.696656	3620.125386	6.493389	-0.030791	3.290731
151.706524	3628.169468	6.498394	-0.030799	3.294182
152.197449	3636.159904	6.503398	-0.030896	3.297624
152.371655	3644.223764	6.508403	-0.030933	3.301082
152.502015	3652.217527	6.513408	-0.030963	3.304505
152.635463	3660.275688	6.518413	-0.030993	3.307951
152.848360	3668.329407	6.523418	-0.031039	3.311396
153.148912	3676.354530	6.528422	-0.031100	3.314827
153.039255	3684.378205	6.533427	-0.031085	3.318239
153.394439	3692.374920	6.538432	-0.031157	3.321654
153.500784	3700.414465	6.543437	-0.031182	3.325074
153.808212	3708.417437	6.548442	-0.031245	3.328482
154.095268	3716.451182	6.553446	-0.031304	3.331899
154.237475	3724.495673	6.558451	-0.031335	3.335312
154.367131	3732.495685	6.563456	-0.031365	3.338702
154.447424	3740.576184	6.568461	-0.031386	3.342120
154.524618	3748.602395	6.573466	-0.031405	3.345512
154.743646	3756.618569	6.578470	-0.031452	3.348902
155.064311	3764.675688	6.583475	-0.031517	3.352309
155.369062	3772.709892	6.588480	-0.031579	3.355702
155.559980	3780.718368	6.593485	-0.031620	3.359077
155.652700	3788.721133	6.598490	-0.031643	3.362442
155.727282	3796.764036	6.603494	-0.031662	3.365821
156.091643	3804.780580	6.608499	-0.031735	3.369195
156.174868	3812.824126	6.613504	-0.031756	3.372567
156.464525	3820.878338	6.618509	-0.031816	3.375948
156.706056	3828.857432	6.623514	-0.031866	3.379292
156.912288	3836.884195	6.628518	-0.031910	3.382651
156.950581	3844.931754	6.633523	-0.031923	3.386010
157.116639	3852.917336	6.638528	-0.031959	3.389344
157.420537	3861.064308	6.643533	-0.032021	3.392746
157.699259	3869.106075	6.648538	-0.032078	3.396101
157.849319	3877.032911	6.653542	-0.032112	3.399400
158.115373	3885.060158	6.658547	-0.032167	3.402741
158.340367	3893.033326	6.663552	-0.032214	3.406056
158.547442	3901.066378	6.668557	-0.032258	3.409391
158.603949	3909.123679	6.673562	-0.032274	3.412728
158.709873	3917.186317	6.678566	-0.032299	3.416065
158.868242	3925.175434	6.683571	-0.032334	3.419371
159.102242	3933.172938	6.688576	-0.032383	3.422679
159.668917	3941.201691	6.693581	-0.032494	3.426008
159.402959	3949.252261	6.698586	-0.032450	3.429315
159.706008	3957.301092	6.703590	-0.032512	3.432637
160.162465	3965.341540	6.708595	-0.032603	3.435958
160.267130	3973.337271	6.713600	-0.032628	3.439245
160.456744	3981.362733	6.718605	-0.032668	3.442544
160.754782	3989.372718	6.723610	-0.032729	3.445837
161.077706	3997.383158	6.728614	-0.032795	3.449128
160.947856	4005.487580	6.733619	-0.032776	3.452439
161.150784	4013.504152	6.738624	-0.032819	3.455722
161.586747	4021.520444	6.743629	-0.032906	3.459010
161.704739	4029.533294	6.748634	-0.032934	3.462282
161.783812	4037.572995	6.753638	-0.032954	3.465561
161.995813	4045.628167	6.758643	-0.032999	3.468848
162.132900	4053.657113	6.763648	-0.033030	3.472118
162.249552	4061.716074	6.768653	-0.033057	3.475397
162.691996	4069.654597	6.773658	-0.033145	3.478634
162.946832	4077.660973	6.778662	-0.033198	3.481890
163.071021	4085.699904	6.783667	-0.033226	3.485151
163.364499	4093.691467	6.788672	-0.033286	3.488396
163.722112	4101.738873	6.793677	-0.033358	3.491662
163.676858	4109.782968	6.798682	-0.033355	3.494911
163.794000	4117.814135	6.803686	-0.033383	3.498157
164.230477	4125.829532	6.808691	-0.033469	3.501404
164.465711	4133.803855	6.813696	-0.033519	3.504624
164.608847	4141.867240	6.818701	-0.033551	3.507875
164.865960	4149.937921	6.823706	-0.033604	3.511129
165.026592	4157.924150	6.828710	-0.033639	3.514343
165.045329	4165.975353	6.833715	-0.033648	3.517576
165.124175	4173.993550	6.838720	-0.033669	3.520795
165.537533	4181.982651	6.843725	-0.033751	3.524009
165.674855	4190.026811	6.848730	-0.033782	3.527233
165.753412	4198.078967	6.853734	-0.033802	3.530456
165.926043	4206.125138	6.858739	-0.033840	3.533677
166.084859	4214.121107	6.863744	-0.033875	3.536874
166.464817	4222.139027	6.868749	-0.033951	3.540084
166.493494	4230.172032	6.873754	-0.033962	3.543286
166.718254	4238.223494	6.878758	-0.034009	3.546499
166.924391	4246.262561	6.883763	-0.034053	3.549703
167.075870	4254.356299	6.888768	-0.034087	3.552924
167.506202	4262.383204	6.893773	-0.034172	3.556124
167.609977	4270.318978	6.898778	-0.034197	3.559276
167.687972	4278.340974	6.903782	-0.034217	3.562458
167.796026	4286.360078	6.908787	-0.034243	3.565636
168.232771	4294.340066	6.913792	-0.034329	3.568807
168.347382	4302.409504	6.918797	-0.034356	3.572000
168.518864	4310.432231	6.923802	-0.034394	3.575173
168.677916	4318.454372	6.928806	-0.034429	3.578343
168.981064	4326.463694	6.933811	-0.034490	3.581510
168.748903	4334.450190	6.938816	-0.034453	3.584649
169.129630	4342.503106	6.943821	-0.034529	3.587829
169.302943	4350.548959	6.948826	-0.034567	3.590997
169.540348	4358.546496	6.953830	-0.034616	3.594146
169.787093	4366.581524	6.958835	-0.034668	3.597307
169.806234	4374.554846	6.963840	-0.034677	3.600434
170.093410	4382.602828	6.968845	-0.034736	3.603595
170.250554	4390.627401	6.973850	-0.034771	3.606741
170.408570	4398.635039	6.978854	-0.034805	3.609877
170.629334	4406.720398	6.983859	-0.034852	3.613043
170.919614	4414.731238	6.988864	-0.034912	3.616179
171.224664	4422.724908	6.993869	-0.034974	3.619306
171.161091	4430.748376	6.998874	-0.034967	3.622431
171.270346	4438.776245	7.003878	-0.034993	3.625560
171.600019	4446.831000	7.008883	-0.035060	3.628703
171.763241	4454.866750	7.013888	-0.035096	3.631831
172.217408	4462.910167	7.018893	-0.035186	3.634968
172.217769	4470.908536	7.023898	-0.035191	3.638072
172.455158	4478.959365	7.028902	-0.035241	3.641200
172.738931	4486.901961	7.033907	-0.035299	3.644284
172.782761	4494.947014	7.038912	-0.035313	3.647399
173.102688	4502.990523	7.043917	-0.035378	3.650518
173.325981	4511.037975	7.048922	-0.035425	3.653634
173.493111	4519.072776	7.053926	-0.035462	3.656740
173.683659	4527.082129	7.058931	-0.035503	3.659835
173.820248	4535.062305	7.063936	-0.035534	3.662914
174.143816	4543.132322	7.068941	-0.035599	3.666030
174.238720	4551.113570	7.073946	-0.035622	3.669103
174.371691	4559.188370	7.078950	-0.035653	3.672211
174.568171	4567.205644	7.083955	-0.035695	3.675296
174.617201	4575.183456	7.088960	-0.035709	3.678359
174.985433	4583.232184	7.093965	-0.035783	3.681454
175.163383	4591.218175	7.098970	-0.035822	3.684519
175.132027	4599.250885	7.103974	-0.035821	3.687593
175.315445	4607.298959	7.108979	-0.035861	3.690676
175.561326	4615.303969	7.113984	-0.035912	3.693741
175.467422	4623.374063	7.118989	-0.035900	3.696821
175.644292	4631.361891	7.123994	-0.035939	3.699873
175.970770	4639.397424	7.128998	-0.036005	3.702944
176.420965	4647.407944	7.134003	-0.036094	3.706006
176.503383	4655.397477	7.139008	-0.036115	3.709049
176.673695	4663.503734	7.144013	-0.036152	3.712136
176.779759	4671.574934	7.149018	-0.036178	3.715205
176.841585	4679.508444	7.154022	-0.036194	3.718218
177.173762	4687.551295	7.159027	-0.036262	3.721277
177.093243	4695.513592	7.164032	-0.036252	3.724293
177.338146	4703.562183	7.169037	-0.036303	3.727347
177.405209	4711.567715	7.174042	-0.036321	3.730378
177.433468	4719.607863	7.179046	-0.036332	3.733419
177.694742	4727.683681	7.184051	-0.036386	3.736476
177.811334	4735.643786	7.189056	-0.036413	3.739483
178.006830	4743.684074	7.194061	-0.036455	3.742520
178.069842	4751.697840	7.199066	-0.036472	3.745542
178.340149	4759.730060	7.204070	-0.036528	3.748572
178.478027	4767.791259	7.209075	-0.036559	3.751609
178.736000	4775.758557	7.214080	-0.036613	3.754610
179.174188	4783.797706	7.219085	-0.036700	3.757640
179.200611	4791.812332	7.224090	-0.036710	3.760648
179.203051	4799.826541	7.229094	-0.036716	3.763654
179.461730	4807.876483	7.234099	-0.036770	3.766676
179.668349	4815.845264	7.239104	-0.036814	3.769665
179.666670	4823.950854	7.244109	-0.036819	3.772697
179.638332	4831.971011	7.249114	-0.036819	3.775694
179.992205	4839.934293	7.254118	-0.036890	3.778677
180.246068	4847.997923	7.259123	-0.036943	3.781692
180.263485	4855.958360	7.264128	-0.036952	3.784661
180.454890	4864.044562	7.269133	-0.036993	3.787679
180.660342	4872.081101	7.274138	-0.037037	3.790675
180.849354	4880.125075	7.279142	-0.037077	3.793672
181.036145	4888.141185	7.284147	-0.037117	3.796656
181.017102	4896.091770	7.289152	-0.037119	3.799609
181.058472	4904.124923	7.294157	-0.037133	3.802591
181.490183	4912.090962	7.299162	-0.037218	3.805555
181.715981	4920.130238	7.304166	-0.037266	3.808539
181.688126	4928.195779	7.309171	-0.037266	3.811525
181.868888	4936.198112	7.314176	-0.037305	3.814490
182.318962	4944.235932	7.319181	-0.037395	3.817471
182.471703	4952.234838	7.324186	-0.037428	3.820429
182.379515	4960.207574	7.329190	-0.037417	3.823370
182.642500	4968.292220	7.334195	-0.037471	3.826357
182.907365	4976.255234	7.339200	-0.037526	3.829298
183.018017	4984.336742	7.344205	-0.037552	3.832276
183.093388	4992.374821	7.349210	-0.037571	3.835235
183.278362	5000.352640	7.354214	-0.037611	3.838173
183.240993	5008.441850	7.359219	-0.037610	3.841144
183.286946	5016.355680	7.364224	-0.037624	3.844050
183.562322	5024.451690	7.369229	-0.037681	3.847026
183.649485	5032.447865	7.374234	-0.037702	3.849959
183.817519	5040.501112	7.379238	-0.037739	3.852912
184.081561	5048.538232	7.384243	-0.037794	3.855858
184.139051	5056.501645	7.389248	-0.037810	3.858772
184.287368	5064.585765	7.394253	-0.037843	3.861729
184.433069	5072.548854	7.399258	-0.037876	3.864640
184.616665	5080.624655	7.404262	-0.037915	3.867590
184.755129	5088.668048	7.409267	-0.037946	3.870525
184.732051	5096.847253	7.414272	-0.037948	3.873505
185.219035	5104.855909	7.419277	-0.038044	3.876430
185.266113	5112.766584	7.424282	-0.038058	3.879308
185.306139	5120.741969	7.429286	-0.038071	3.882208
185.515303	5128.735797	7.434291	-0.038115	3.885115
185.784786	5136.745406	7.439296	-0.038171	3.888028
185.768763	5144.787489	7.444301	-0.038173	3.890944
185.966860	5152.829457	7.449306	-0.038216	3.893862
186.106672	5160.813347	7.454310	-0.038247	3.896756
186.365589	5168.806483	7.459315	-0.038301	3.899653
186.495932	5176.812404	7.464320	-0.038331	3.902550
186.608194	5184.860721	7.469325	-0.038357	3.905460
186.898352	5192.898944	7.474330	-0.038416	3.908368
186.876574	5200.927381	7.479334	-0.038418	3.911264
187.142117	5208.954765	7.484339	-0.038473	3.914162
187.500052	5216.928858	7.489344	-0.038545	3.917042
187.902406	5224.932738	7.494349	-0.038625	3.919930
187.683869	5232.960426	7.499354	-0.038590	3.922814
187.905121	5240.958591	7.504358	-0.038637	3.925692
188.165643	5248.983353	7.509363	-0.038691	3.928579
188.134381	5257.053191	7.514368	-0.038690	3.931475
188.395906	5265.064653	7.519373	-0.038744	3.934353
188.490524	5273.079107	7.524378	-0.038768	3.937227
188.548616	5281.057675	7.529382	-0.038784	3.940085
188.503048	5289.120520	7.534387	-0.038781	3.942969
188.748863	5297.132947	7.539392	-0.038832	3.945839
188.985008	5305.150047	7.544397	-0.038881	3.948707
188.931293	5313.212649	7.549402	-0.038877	3.951585
189.424970	5321.214144	7.554406	-0.038974	3.954449
189.602832	5329.255397	7.559411	-0.039013	3.957319
189.601331	5337.201674	7.564416	-0.039018	3.960150
189.931592	5345.249063	7.569421	-0.039085	3.963021
189.902412	5353.244192	7.574426	-0.039085	3.965864
189.999643	5361.238132	7.579430	-0.039109	3.968708
190.092946	5369.336507	7.584435	-0.039131	3.971586
190.208923	5377.341193	7.589440	-0.039158	3.974430
190.477821	5385.383184	7.594445	-0.039214	3.977287
190.545365	5393.370947	7.599450	-0.039232	3.980120
190.808174	5401.359698	7.604454	-0.039286	3.982954
190.948216	5409.416454	7.609459	-0.039318	3.985808
190.941001	5417.386117	7.614464	-0.039322	3.988627
191.273878	5425.468510	7.619469	-0.039390	3.991489
191.378364	5433.526699	7.624474	-0.039414	3.994337
191.629259	5441.506108	7.629478	-0.039467	3.997158
191.780681	5449.533885	7.634483	-0.039500	3.999991
191.904866	5457.540310	7.639488	-0.039529	4.002815
192.143732	5465.562330	7.644493	-0.039579	4.005644
192.052381	5473.591708	7.649498	-0.039567	4.008469
192.243795	5481.638001	7.654502	-0.039608	4.011302
192.425443	5489.694061	7.659507	-0.039648	4.014136
192.476639	5497.662996	7.664512	-0.039663	4.016935
192.552870	5505.683574	7.669517	-0.039682	4.019751
192.802854	5513.691465	7.674522	-0.039734	4.022564
192.764329	5521.688337	7.679526	-0.039733	4.025366
193.056442	5529.725361	7.684531	-0.039792	4.028185
193.174723	5537.779284	7.689536	-0.039820	4.031005
193.380057	5545.886928	7.694541	-0.039864	4.033844
193.546402	5553.887671	7.699546	-0.039900	4.036642
193.601744	5561.798651	7.704550	-0.039916	4.039406
193.791393	5569.836412	7.709555	-0.039957	4.042214
193.895235	5577.786785	7.714560	-0.039981	4.044988
194.034724	5585.844213	7.719565	-0.040013	4.047798
194.269999	5593.885332	7.724570	-0.040062	4.050602
194.328160	5601.889309	7.729574	-0.040078	4.053389
194.377315	5609.936021	7.734579	-0.040093	4.056188
194.608470	5617.878306	7.739584	-0.040141	4.058951
194.840761	5625.941166	7.744589	-0.040190	4.061755
194.811119	5633.948502	7.749594	-0.040190	4.064533
194.993926	5641.968810	7.754598	-0.040230	4.067318
195.383406	5649.987166	7.759603	-0.040308	4.070102
195.392362	5658.022128	7.764608	-0.040315	4.072885
195.198611	5666.075303	7.769613	-0.040284	4.075670
195.515312	5674.044753	7.774618	-0.040348	4.078430
195.622735	5682.023603	7.779622	-0.040374	4.081190
195.731672	5690.067521	7.784627	-0.040400	4.083969
196.012558	5698.123729	7.789632	-0.040457	4.086754
196.284132	5706.097191	7.794637	-0.040513	4.089508
196.158095	5714.145213	7.799642	-0.040495	4.092280
196.297752	5722.158349	7.804646	-0.040527	4.095042
196.610681	5730.210149	7.809651	-0.040591	4.097818
196.685569	5738.173249	7.814656	-0.040610	4.100558
196.654440	5746.201213	7.819661	-0.040610	4.103317
197.179963	5754.246905	7.824666	-0.040713	4.106088
197.337274	5762.261334	7.829670	-0.040748	4.108842
197.477798	5770.326458	7.834675	-0.040779	4.111610
197.699980	5778.332058	7.839680	-0.040826	4.114357
197.778093	5786.353981	7.844685	-0.040846	4.117107
197.893500	5794.357109	7.849690	-0.040873	4.119848
197.774706	5802.364275	7.854694	-0.040857	4.122586
198.025194	5810.381357	7.859699	-0.040909	4.125330
198.314834	5818.376859	7.864704	-0.040968	4.128066
198.408460	5826.446234	7.869709	-0.040991	4.130822
198.473621	5834.501028	7.874714	-0.041009	4.133572
198.633019	5842.495534	7.879718	-0.041044	4.136300
198.910894	5850.480135	7.884723	-0.041101	4.139024
198.620689	5858.530781	7.889728	-0.041052	4.141762
199.062712	5866.511050	7.894733	-0.041140	4.144483
199.404502	5874.565499	7.899738	-0.041209	4.147226
199.511281	5882.571208	7.904742	-0.041234	4.149948
199.737792	5890.649762	7.909747	-0.041282	4.152695
199.761373	5898.608321	7.914752	-0.041292	4.155396
199.878065	5906.625943	7.919757	-0.041319	4.158117
200.139511	5914.641130	7.924762	-0.041373	4.160837
200.251080	5922.617938	7.929766	-0.041399	4.163540
200.267951	5930.704686	7.934771	-0.041408	4.166278
200.487325	5938.689297	7.939776	-0.041454	4.168982
200.853628	5946.746306	7.944781	-0.041528	4.171710
200.837851	5954.774370	7.949786	-0.041531	4.174422
200.821095	5962.775314	7.954790	-0.041533	4.177123
201.192179	5970.776034	7.959795	-0.041607	4.179827
201.548494	5978.775171	7.964800	-0.041679	4.182528
201.619605	5986.806549	7.969805	-0.041698	4.185235
201.601397	5994.833078	7.974810	-0.041700	4.187937
201.728590	6002.822056	7.979814	-0.041729	4.190627
202.092783	6010.987853	7.984819	-0.041803	4.193378
202.155710	6018.962478	7.989824	-0.041820	4.196058
202.331406	6026.873579	7.994829	-0.041858	4.198717
202.558374	6034.941678	7.999834	-0.041906	4.201428
202.769314	6042.828455	8.004838	-0.041950	4.204076
202.795774	6050.944960	8.009843	-0.041961	4.206797
202.859533	6058.921093	8.014848	-0.041978	4.209470
203.110774	6066.970268	8.019853	-0.042030	4.212167
203.242696	6075.007816	8.024858	-0.042060	4.214858
203.491532	6082.988177	8.029862	-0.042112	4.217528
203.788027	6091.019937	8.034867	-0.042173	4.220215
203.617422	6099.001709	8.039872	-0.042146	4.222879
204.065719	6107.038382	8.044877	-0.042235	4.225565
204.071612	6115.050346	8.049882	-0.042242	4.228238
203.903512	6123.079987	8.054886	-0.042216	4.230912
204.178021	6131.158010	8.059891	-0.042273	4.233606
204.429711	6139.131251	8.064896	-0.042325	4.236262
204.752028	6147.120720	8.069901	-0.042390	4.238923
204.693083	6155.146898	8.074906	-0.042385	4.241591
204.974212	6163.084813	8.079910	-0.042443	4.244231
205.257903	6171.166925	8.084915	-0.042501	4.246917
205.275968	6179.166647	8.089920	-0.042510	4.249571
205.229181	6187.244762	8.094925	-0.042507	4.252250
205.514410	6195.276397	8.099930	-0.042565	4.254914
205.604892	6203.260059	8.104934	-0.042587	4.257559
205.887007	6211.305795	8.109939	-0.042645	4.260225
205.965774	6219.290427	8.114944	-0.042666	4.262866
206.218031	6227.318860	8.119949	-0.042718	4.265523
206.107861	6235.354487	8.124954	-0.042703	4.268176
206.091100	6243.371801	8.129958	-0.042705	4.270823
206.466993	6251.435855	8.134963	-0.042781	4.273487
206.521571	6259.452848	8.139968	-0.042796	4.276131
206.638985	6267.443832	8.144973	-0.042824	4.278766
207.014171	6275.485344	8.149978	-0.042899	4.281417
206.978637	6283.409607	8.154982	-0.042898	4.284025
207.121462	6291.506040	8.159987	-0.042930	4.286689
207.298961	6299.470852	8.164992	-0.042968	4.289309
207.343854	6307.545624	8.169997	-0.042982	4.291962
207.452401	6315.577241	8.175002	-0.043008	4.294600
207.657062	6323.543918	8.180006	-0.043051	4.297215
207.792883	6331.590543	8.185011	-0.043082	4.299855
207.910972	6339.568271	8.190016	-0.043110	4.302470
207.981737	6347.578739	8.195021	-0.043128	4.305094
208.212462	6355.636140	8.200026	-0.043177	4.307733
208.327114	6363.615385	8.205030	-0.043203	4.310344
208.332803	6371.715742	8.210035	-0.043210	4.312992
208.525105	6379.695378	8.215040	-0.043251	4.315601
208.958136	6387.632327	8.220045	-0.043337	4.318196
208.839240	6395.728413	8.225050	-0.043321	4.320836
208.910997	6403.665192	8.230054	-0.043339	4.323425
209.144527	6411.774676	8.235059	-0.043388	4.326070
209.002001	6419.743176	8.240064	-0.043367	4.328664
209.276381	6427.753314	8.245069	-0.043424	4.331274
209.531414	6435.812021	8.250074	-0.043477	4.333897
209.700501	6443.815136	8.255078	-0.043514	4.336500
209.647981	6451.801916	8.260083	-0.043509	4.339095
209.958554	6459.823290	8.265088	-0.043573	4.341702
210.072269	6467.830648	8.270093	-0.043599	4.344301
210.115588	6475.868390	8.275098	-0.043613	4.346908
210.060884	6483.887950	8.280102	-0.043608	4.349507
210.593274	6491.955280	8.285107	-0.043713	4.352124
210.641510	6500.010449	8.290112	-0.043727	4.354732
210.731495	6507.971188	8.295117	-0.043749	4.357309
210.832641	6515.977025	8.300122	-0.043774	4.359898
211.081670	6523.947083	8.305126	-0.043825	4.362475
211.047180	6531.932298	8.310131	-0.043824	4.365054
211.107807	6539.964908	8.315136	-0.043841	4.367647
211.393954	6548.003844	8.320141	-0.043900	4.370242
211.559900	6556.036381	8.325146	-0.043936	4.372833
211.778024	6564.056308	8.330150	-0.043982	4.375418
211.896078	6572.066431	8.335155	-0.044010	4.377998
211.883378	6580.031317	8.340160	-0.044013	4.380561
212.300222	6588.049436	8.345165	-0.044096	4.383143
212.452631	6596.094665	8.350170	-0.044130	4.385729
212.467714	6604.130612	8.355174	-0.044138	4.388311
212.728631	6612.192303	8.360179	-0.044192	4.390901
212.705527	6620.165467	8.365184	-0.044193	4.393459
212.925390	6628.197561	8.370189	-0.044240	4.396036
213.139265	6636.218974	8.375194	-0.044285	4.398608
213.041766	6644.212344	8.380198	-0.044272	4.401167
213.471442	6652.217254	8.385203	-0.044358	4.403732
213.568375	6660.213884	8.390208	-0.044381	4.406291
213.701472	6668.230255	8.395213	-0.044411	4.408855
213.833564	6676.286552	8.400218	-0.044442	4.411430
214.028786	6684.292842	8.405222	-0.044483	4.413988
214.077228	6692.386372	8.410227	-0.044498	4.416571
214.117140	6700.341862	8.415232	-0.044511	4.419109
214.371810	6708.377068	8.420237	-0.044564	4.421672
214.610656	6716.389837	8.425242	-0.044614	4.424226
214.473345	6724.417785	8.430246	-0.044593	4.426782
214.822041	6732.430503	8.435251	-0.044664	4.429333
214.848374	6740.463413	8.440256	-0.044674	4.431888
214.977900	6748.519166	8.445261	-0.044704	4.434450
215.272509	6756.528183	8.450266	-0.044764	4.436995
215.489571	6764.462337	8.455270	-0.044810	4.439515
215.534482	6772.539240	8.460275	-0.044824	4.442079
215.493030	6780.485114	8.465280	-0.044822	4.444598
215.728778	6788.552039	8.470285	-0.044871	4.447156
215.973825	6796.544723	8.475290	-0.044922	4.449689
216.002916	6804.575405	8.480294	-0.044933	4.452232
216.305331	6812.644762	8.485299	-0.044995	4.454786
216.276951	6820.613362	8.490304	-0.044995	4.457306
216.536886	6828.588877	8.495309	-0.045049	4.459827
216.646418	6836.645963	8.500314	-0.045074	4.462373
216.878814	6844.600399	8.505318	-0.045123	4.464885
217.199351	6852.679149	8.510323	-0.045188	4.467435
217.214700	6860.654222	8.515328	-0.045197	4.469950
217.295465	6868.704414	8.520333	-0.045217	4.472487
217.525207	6876.750634	8.525338	-0.045265	4.475022
217.860763	6884.729930	8.530342	-0.045333	4.477535
217.987805	6892.754783	8.535347	-0.045362	4.480060
218.098490	6900.744664	8.540352	-0.045388	4.482572
218.328231	6908.738852	8.545357	-0.045437	4.485085
218.426136	6916.764801	8.550362	-0.045460	4.487606
218.543821	6924.783176	8.555366	-0.045488	4.490124
218.677996	6932.865674	8.560371	-0.045518	4.492660
218.653808	6940.871630	8.565376	-0.045519	4.495170
218.867975	6948.861910	8.570381	-0.045565	4.497674
219.096374	6956.880537	8.575386	-0.045613	4.500186
219.163530	6964.859283	8.580391	-0.045630	4.502684
219.169944	6972.886945	8.585395	-0.045637	4.505195
219.485798	6980.896489	8.590400	-0.045701	4.507700
219.494175	6988.947155	8.595405	-0.045708	4.510216
219.408784	6997.044086	8.600410	-0.045698	4.512744
219.661685	7005.015790	8.605415	-0.045751	4.515233
219.978305	7013.008526	8.610419	-0.045815	4.517727
219.975081	7020.953131	8.615424	-0.045820	4.520204
220.041403	7028.960718	8.620429	-0.045838	4.522700
220.324674	7037.005304	8.625434	-0.045896	4.525206
220.320877	7045.031382	8.630439	-0.045901	4.527704
220.437475	7053.046030	8.635443	-0.045928	4.530198
220.576093	7061.063998	8.640448	-0.045959	4.532691
220.672706	7069.062591	8.645453	-0.045982	4.535177
220.717728	7077.115208	8.650458	-0.045996	4.537678
220.763444	7085.066652	8.655463	-0.046010	4.540146
220.982572	7093.114055	8.660467	-0.046056	4.542643
220.927458	7101.101039	8.665472	-0.046052	4.545119
221.384299	7109.159138	8.670477	-0.046142	4.547617
221.718528	7117.188210	8.675482	-0.046210	4.550104
221.705809	7125.203374	8.680487	-0.046213	4.552586
221.784503	7133.268907	8.685491	-0.046233	4.555081
221.916863	7141.248768	8.690496	-0.046263	4.557549
222.103604	7149.252983	8.695501	-0.046303	4.560022
222.170458	7157.258089	8.700506	-0.046321	4.562495
222.252726	7165.238173	8.705511	-0.046342	4.564959
222.566998	7173.295605	8.710515	-0.046406	4.567445
222.610288	7181.281580	8.715520	-0.046420	4.569908
222.693121	7189.339639	8.720525	-0.046440	4.572391
223.062884	7197.396120	8.725530	-0.046515	4.574873
223.137302	7205.358622	8.730535	-0.046534	4.577325
223.378160	7213.410207	8.735539	-0.046584	4.579802
223.375797	7221.400896	8.740544	-0.046589	4.582260
223.446817	7229.405861	8.745549	-0.046608	4.584720
223.390032	7237.451034	8.750554	-0.046603	4.587191
223.505602	7245.429990	8.755559	-0.046630	4.589641
223.666214	7253.519016	8.760563	-0.046665	4.592124
223.793228	7261.566727	8.765568	-0.046694	4.594592
223.961016	7269.521978	8.770573	-0.046731	4.597030
224.182436	7277.505921	8.775578	-0.046778	4.599476
223.994385	7285.517099	8.780583	-0.046748	4.601929
224.372396	7293.529928	8.785587	-0.046824	4.604382
224.585921	7301.584057	8.790592	-0.046869	4.606845
224.705101	7309.534358	8.795597	-0.046897	4.609276
224.658549	7317.635120	8.800602	-0.046894	4.611751
224.819192	7325.603166	8.805607	-0.046929	4.614184
225.098594	7333.705435	8.810611	-0.046987	4.616657
224.968171	7341.621654	8.815616	-0.046968	4.619072
225.145779	7349.668092	8.820621	-0.047006	4.621525
225.357568	7357.626673	8.825626	-0.047051	4.623950
225.212934	7365.666126	8.830631	-0.047030	4.626399
225.415075	7373.686551	8.835635	-0.047073	4.628840
225.494494	7381.724491	8.840640	-0.047093	4.631286
225.569503	7389.780063	8.845645	-0.047112	4.633735
225.608744	7397.815217	8.850650	-0.047125	4.636177
225.781356	7405.724309	8.855655	-0.047163	4.638580
225.929876	7413.757873	8.860659	-0.047196	4.641019
226.199700	7421.767179	8.865664	-0.047252	4.643449
226.414028	7429.771394	8.870669	-0.047297	4.645876
226.580391	7437.804488	8.875674	-0.047333	4.648311
226.574410	7445.810465	8.880679	-0.047338	4.650737
226.729822	7453.940740	8.885683	-0.047372	4.653198
226.782931	7461.898616	8.890688	-0.047388	4.655607
226.944515	7469.867201	8.895693	-0.047423	4.658017
226.989252	7477.896379	8.900698	-0.047437	4.660444
227.047032	7485.866775	8.905703	-0.047453	4.662853
227.239854	7493.915271	8.910707	-0.047494	4.665283
227.264549	7501.914588	8.915712	-0.047504	4.667698
227.333307	7509.929643	8.920717	-0.047523	4.670116
227.547327	7518.096605	8.925722	-0.047568	4.672578
227.797855	7526.095096	8.930727	-0.047620	4.674988
227.820601	7534.074928	8.935731	-0.047630	4.677392
228.089329	7542.008275	8.940736	-0.047685	4.679780
228.347983	7550.057816	8.945741	-0.047739	4.682201
228.195505	7558.017996	8.950746	-0.047716	4.684596
228.331669	7566.071107	8.955751	-0.047747	4.687016
228.564334	7574.045858	8.960755	-0.047796	4.689412
228.543577	7582.097078	8.965760	-0.047797	4.691829
228.871384	7590.104698	8.970765	-0.047864	4.694232
228.894486	7598.162469	8.975770	-0.047873	4.696649
228.956203	7606.093428	8.980775	-0.047890	4.699027
229.088380	7614.133130	8.985779	-0.047920	4.701436
229.097985	7622.132358	8.990784	-0.047928	4.703832
229.234576	7630.190843	8.995789	-0.047959	4.706244
229.577262	7638.184085	9.000794	-0.048028	4.708634
229.467777	7646.226110	9.005799	-0.048013	4.711040
229.575936	7654.248842	9.010803	-0.048039	4.713437
229.666654	7662.247346	9.015808	-0.048061	4.715827
229.730854	7670.254960	9.020813	-0.048078	4.718217
229.975133	7678.272370	9.025818	-0.048129	4.720610
230.044911	7686.257898	9.030823	-0.048148	4.722991
230.189514	7694.302619	9.035827	-0.048180	4.725389
230.309504	7702.306205	9.040832	-0.048208	4.727774
230.470597	7710.340477	9.045837	-0.048243	4.730166
230.600668	7718.427902	9.050842	-0.048273	4.732573
230.660873	7726.386584	9.055847	-0.048290	4.734941
231.138058	7734.440522	9.060851	-0.048384	4.737335
231.052115	7742.388038	9.065856	-0.048373	4.739697
231.009153	7750.406157	9.070861	-0.048371	4.742079
231.028712	7758.405810	9.075866	-0.048380	4.744454
231.041138	7766.459921	9.080871	-0.048388	4.746845
231.460361	7774.457206	9.085875	-0.048471	4.749216
231.297131	7782.510212	9.090880	-0.048446	4.751604
231.686921	7790.518578	9.095885	-0.048524	4.753975
231.763832	7798.577109	9.100890	-0.048544	4.756362
231.916159	7806.503457	9.105895	-0.048578	4.758708
231.970057	7814.520229	9.110899	-0.048593	4.761079
232.179593	7822.531267	9.115904	-0.048638	4.763448
232.424435	7830.529905	9.120909	-0.048689	4.765811
232.413688	7838.565407	9.125914	-0.048692	4.768185
232.377275	7846.561238	9.130919	-0.048691	4.770546
232.671702	7854.651989	9.135923	-0.048751	4.772933
232.779746	7862.662994	9.140928	-0.048777	4.775296
233.051790	7870.629325	9.145933	-0.048833	4.777644
232.875238	7878.663665	9.150938	-0.048806	4.780012
233.033391	7886.654493	9.155943	-0.048841	4.782365
233.261575	7894.696954	9.160947	-0.048888	4.784732
233.316162	7902.711371	9.165952	-0.048904	4.787090
233.348781	7910.684864	9.170957	-0.048916	4.789435
233.451406	7918.769515	9.175962	-0.048940	4.791811
233.623714	7926.758264	9.180967	-0.048978	4.794157
233.978766	7934.825987	9.185971	-0.049049	4.796525
234.003698	7942.757827	9.190976	-0.049059	4.798853
234.132211	7950.803663	9.195981	-0.049089	4.801213
234.548681	7958.786551	9.200986	-0.049172	4.803552
234.245602	7966.787967	9.205991	-0.049121	4.805899
234.287567	7974.808171	9.210995	-0.049134	4.808248
234.642793	7982.871404	9.216000	-0.049206	4.810607
234.739436	7990.247440	9.221005	-0.049229	4.812765
234.749121	7994.818198	9.226010	-0.049234	4.814103

234.797937	7997.190706	9.231015	-0.049245	4.814796
235.015555	7998.536090	9.236019	-0.049286	4.815189
235.001655	7998.969313	9.241024	-0.049284	4.815316
235.096643	7999.834562	9.246029	-0.049303	4.815568
235.102687	7999.824004	9.251034	-0.049304	4.815565
235.027753	7999.813199	9.256039	-0.049290	4.815562
235.164741	7999.823984	9.261043	-0.049316	4.815565
235.381453	7999.804033	9.266048	-0.049357	4.815558
235.430281	7999.822996	9.271053	-0.049366	4.815563
235.450149	7999.837218	9.276058	-0.049370	4.815567
235.419032	7999.785486	9.281063	-0.049364	4.815552
235.582920	7999.827669	9.286067	-0.049395	4.815564
235.398839	7999.833243	9.291072	-0.049361	4.815566
235.527556	7999.864179	9.296077	-0.049385	4.815575
235.814789	7999.852847	9.301082	-0.049439	4.815570
235.703962	7999.812633	9.306087	-0.049418	4.815559
235.683847	7999.843289	9.311091	-0.049415	4.815568
235.945730	7999.821937	9.316096	-0.049464	4.815560
235.784328	7999.822540	9.321101	-0.049434	4.815561
235.684388	7999.845493	9.326106	-0.049416	4.815568
235.772192	7999.836263	9.331111	-0.049432	4.815565
235.868028	7999.845312	9.336115	-0.049450	4.815567
235.844773	7999.815061	9.341120	-0.049446	4.815559
235.832690	7999.856523	9.346125	-0.049444	4.815571
235.882206	7999.821047	9.351130	-0.049454	4.815560
235.965231	7999.822416	9.356135	-0.049469	4.815560
236.018864	7999.845727	9.361139	-0.049480	4.815567
236.124427	7999.837853	9.366144	-0.049500	4.815564
236.285676	7999.833017	9.371149	-0.049530	4.815562
236.072524	7999.858404	9.376154	-0.049490	4.815570
236.207431	7999.834991	9.381159	-0.049516	4.815563
236.592757	7999.851944	9.386163	-0.049588	4.815566
236.264069	7999.817801	9.391168	-0.049527	4.815557
236.159084	7999.837469	9.396173	-0.049507	4.815564
236.456393	7999.844453	9.401178	-0.049563	4.815564
236.491299	7999.829025	9.406183	-0.049570	4.815560
236.245977	7999.846415	9.411187	-0.049524	4.815566
236.240562	7999.823926	9.416192	-0.049524	4.815559
236.323715	7999.833838	9.421197	-0.049539	4.815562
236.359156	7999.867531	9.426202	-0.049546	4.815572
236.388879	7999.813583	9.431207	-0.049552	4.815556
236.655009	7999.843549	9.436211	-0.049602	4.815563
236.475595	7999.825709	9.441216	-0.049568	4.815559
236.420627	7999.844054	9.446221	-0.049558	4.815564
236.609638	7999.841806	9.451226	-0.049594	4.815563
236.598721	7999.834175	9.456231	-0.049592	4.815561
236.665311	7999.868375	9.461235	-0.049605	4.815570
236.708917	7999.837073	9.466240	-0.049613	4.815561
236.703375	7999.850883	9.471245	-0.049612	4.815565
236.661468	7999.850223	9.476250	-0.049605	4.815565
236.606047	7999.818381	9.481255	-0.049595	4.815556
236.765295	7999.846611	9.486259	-0.049625	4.815563
236.448695	7999.824407	9.491264	-0.049566	4.815558
236.452341	7999.825554	9.496269	-0.049567	4.815559
236.583980	7999.852269	9.501274	-0.049591	4.815566
236.657343	7999.807571	9.506279	-0.049605	4.815552
236.615623	7999.865635	9.511283	-0.049598	4.815570
236.633595	7999.853135	9.516288	-0.049601	4.815566
236.718911	7999.836391	9.521293	-0.049618	4.815561
236.826730	7999.872328	9.526298	-0.049638	4.815571
236.658075	7999.849323	9.531303	-0.049607	4.815565
236.785538	7999.879173	9.536307	-0.049631	4.815573
236.915771	7999.866361	9.541312	-0.049655	4.815568
236.652953	7999.837556	9.546317	-0.049606	4.815561
236.796078	7999.838833	9.551322	-0.049633	4.815561
236.903897	7999.829928	9.556327	-0.049654	4.815558
236.778965	7999.845002	9.561331	-0.049631	4.815563
236.742713	7999.838028	9.566336	-0.049624	4.815561
236.983290	7999.855835	9.571341	-0.049669	4.815565
237.132699	7999.858282	9.576346	-0.049697	4.815565
236.944973	7999.834967	9.581351	-0.049662	4.815559
236.943948	7999.845648	9.586355	-0.049662	4.815562
237.175034	7999.843016	9.591360	-0.049706	4.815560
236.882951	7999.859645	9.596365	-0.049652	4.815567
237.073638	7999.864898	9.601370	-0.049687	4.815567
237.211213	7999.850070	9.606375	-0.049713	4.815562
236.951712	7999.861891	9.611379	-0.049665	4.815567
237.064871	7999.846666	9.616384	-0.049686	4.815562
237.186923	7999.858278	9.621389	-0.049709	4.815565
237.145368	7999.861894	9.626394	-0.049702	4.815566
237.023669	7999.851396	9.631399	-0.049679	4.815563
237.337339	7999.869324	9.636403	-0.049738	4.815567
237.367930	7999.829269	9.641408	-0.049744	4.815555
237.206288	7999.838408	9.646413	-0.049714	4.815559
237.154105	7999.847190	9.651418	-0.049705	4.815562
237.161799	7999.829185	9.656423	-0.049706	4.815556
237.144851	7999.860960	9.661427	-0.049703	4.815566
237.263365	7999.857567	9.666432	-0.049726	4.815564
237.191257	7999.840401	9.671437	-0.049712	4.815559
237.132536	7999.838400	9.676442	-0.049702	4.815559
236.983551	7999.824256	9.681447	-0.049674	4.815556
237.144770	7999.865331	9.686451	-0.049704	4.815567
237.220300	7999.845225	9.691456	-0.049719	4.815561
237.152099	7999.849475	9.696461	-0.049706	4.815562
237.232700	7999.870023	9.701466	-0.049722	4.815568
237.373302	7999.836026	9.706471	-0.049748	4.815557
237.399990	7999.848225	9.711475	-0.049753	4.815561
237.384021	7999.839444	9.716480	-0.049750	4.815558
237.394036	7999.847101	9.721485	-0.049753	4.815560
237.324327	7999.848124	9.726490	-0.049740	4.815561
237.206520	7999.825945	9.731495	-0.049718	4.815555
237.066798	7999.867471	9.736499	-0.049692	4.815568
237.300632	7999.873425	9.741504	-0.049736	4.815568
237.356402	7999.870080	9.746509	-0.049747	4.815567
237.418193	7999.867901	9.751514	-0.049758	4.815566
237.152037	7999.834770	9.756519	-0.049709	4.815558
237.346478	7999.882792	9.761523	-0.049746	4.815571
237.461411	7999.854785	9.766528	-0.049767	4.815562
237.314769	7999.852422	9.771533	-0.049740	4.815562
237.431982	7999.884242	9.776538	-0.049762	4.815571
237.444183	7999.858836	9.781543	-0.049765	4.815563
237.514660	7999.882423	9.786547	-0.049778	4.815570
237.388643	7999.863313	9.791552	-0.049755	4.815565
237.463705	7999.864553	9.796557	-0.049769	4.815565
237.312920	7999.870665	9.801562	-0.049741	4.815567
237.303976	7999.853457	9.806567	-0.049740	4.815562
237.410077	7999.878690	9.811571	-0.049760	4.815569
237.420160	7999.859656	9.816576	-0.049762	4.815564
237.279794	7999.868073	9.821581	-0.049736	4.815567
237.659121	7999.869985	9.826586	-0.049807	4.815566
237.576507	7999.830226	9.831591	-0.049792	4.815554
237.514582	7999.882625	9.836595	-0.049780	4.815570
237.483476	7999.857583	9.841600	-0.049775	4.815563
237.345561	7999.816926	9.846605	-0.049749	4.815552
237.382028	7999.849569	9.851610	-0.049756	4.815561
237.339226	7999.835014	9.856615	-0.049749	4.815557
237.485345	7999.864101	9.861619	-0.049776	4.815565
237.553828	7999.858827	9.866624	-0.049789	4.815563
237.480728	7999.855525	9.871629	-0.049776	4.815562
237.654017	7999.869037	9.876634	-0.049808	4.815565
237.460774	7999.820007	9.881639	-0.049772	4.815552
237.447785	7999.835832	9.886643	-0.049770	4.815557
237.541140	7999.835233	9.891648	-0.049788	4.815556
237.452232	7999.819929	9.896653	-0.049771	4.815552
237.444235	7999.824091	9.901658	-0.049770	4.815553
237.404015	7999.842676	9.906663	-0.049763	4.815559
237.620278	7999.868631	9.911667	-0.049804	4.815565
237.738165	7999.857755	9.916672	-0.049826	4.815562
237.447474	7999.850917	9.921677	-0.049772	4.815561
237.525241	7999.827643	9.926682	-0.049786	4.815554
237.487735	7999.789685	9.931687	-0.049780	4.815543
237.653633	7999.848989	9.936691	-0.049811	4.815559
237.687457	7999.820731	9.941696	-0.049817	4.815551
237.645726	7999.829682	9.946701	-0.049810	4.815554
237.723168	7999.846976	9.951706	-0.049825	4.815558
237.632464	7999.835913	9.956711	-0.049808	4.815556
237.641529	7999.883060	9.961715	-0.049810	4.815569
237.598701	7999.853556	9.966720	-0.049802	4.815561
237.569537	7999.857374	9.971725	-0.049797	4.815562
237.747347	7999.874163	9.976730	-0.049830	4.815566
237.498308	7999.853054	9.981735	-0.049784	4.815561
237.490858	7999.873239	9.986739	-0.049783	4.815567
237.505094	7999.850002	9.991744	-0.049786	4.815560
237.629665	7999.853114	9.996749	-0.049809	4.815561
237.592480	7999.842920	10.001754	-0.049802	4.815558
237.633161	7999.831857	10.006759	-0.049810	4.815554
237.630497	7999.861730	10.011763	-0.049810	4.815563
237.730427	7999.846290	10.016768	-0.049829	4.815558
237.698362	7999.870347	10.021773	-0.049823	4.815565
237.881176	7999.879744	10.026778	-0.049857	4.815567
237.839501	7999.842785	10.031783	-0.049850	4.815557
237.728756	7999.861292	10.036787	-0.049830	4.815562
237.761936	7999.837295	10.041792	-0.049836	4.815555
237.719000	7999.883596	10.046797	-0.049828	4.815569
237.774257	7999.877040	10.051802	-0.049839	4.815567
237.740030	7999.860489	10.056807	-0.049833	4.815562
237.776010	7999.852552	10.061811	-0.049839	4.815560
237.691439	7999.833048	10.066816	-0.049824	4.815554
237.647650	7999.846236	10.071821	-0.049816	4.815558
237.771000	7999.868547	10.076826	-0.049839	4.815564
237.903684	7999.844031	10.081831	-0.049864	4.815557
237.899328	7999.870673	10.086835	-0.049864	4.815564
238.018120	7999.855541	10.091840	-0.049886	4.815559
237.877125	7999.834051	10.096845	-0.049860	4.815554
237.863211	7999.874418	10.101850	-0.049858	4.815566
237.583650	7999.831459	10.106855	-0.049806	4.815554
238.007291	7999.859717	10.111859	-0.049885	4.815561
237.810505	7999.835185	10.116864	-0.049848	4.815554
237.793956	7999.849884	10.121869	-0.049846	4.815559
237.862903	7999.876650	10.126874	-0.049859	4.815566
237.723428	7999.825290	10.131879	-0.049833	4.815552
237.814365	7999.834261	10.136883	-0.049850	4.815554
237.815316	7999.834297	10.141888	-0.049851	4.815554
237.986741	7999.856322	10.146893	-0.049883	4.815560
238.073214	7999.868424	10.151898	-0.049899	4.815563
238.011232	7999.839677	10.156903	-0.049888	4.815555
237.973296	7999.879654	10.161907	-0.049881	4.815567
237.973476	7999.852984	10.166912	-0.049881	4.815559
237.926008	7999.854369	10.171917	-0.049873	4.815559
238.144520	7999.873956	10.176922	-0.049913	4.815564
238.099709	7999.857232	10.181927	-0.049905	4.815559
237.879944	7999.863290	10.186931	-0.049865	4.815562
237.923412	7999.849069	10.191936	-0.049873	4.815558
237.976110	7999.855284	10.196941	-0.049883	4.815559
238.056392	7999.861948	10.201946	-0.049898	4.815561
237.980276	7999.852190	10.206951	-0.049884	4.815558
238.115096	7999.853333	10.211955	-0.049910	4.815558
238.209615	7999.871973	10.216960	-0.049927	4.815563
238.097751	7999.880852	10.221965	-0.049907	4.815566
238.051499	7999.864105	10.226970	-0.049898	4.815562
237.996550	7999.847217	10.231975	-0.049888	4.815557
238.006457	7999.885836	10.236979	-0.049891	4.815568
237.962888	7999.843507	10.241984	-0.049883	4.815556
237.844568	7999.825590	10.246989	-0.049861	4.815551
237.970954	7999.886388	10.251994	-0.049885	4.815568
237.676651	7999.856000	10.256999	-0.049830	4.815561
237.840910	7999.837336	10.262003	-0.049861	4.815555
237.971648	7999.934507	10.267008	-0.049885	4.815582
238.035078	7999.823448	10.272013	-0.049897	4.815550
238.090930	7999.863882	10.277018	-0.049908	4.815561
238.177260	7999.841815	10.282023	-0.049924	4.815554
238.205022	7999.861506	10.287027	-0.049930	4.815560
238.169204	7999.865215	10.292032	-0.049923	4.815561
238.214446	7999.868106	10.297037	-0.049932	4.815562
238.192625	7999.877381	10.302042	-0.049928	4.815565
237.899999	7999.832072	10.307047	-0.049874	4.815553
237.985914	7999.838827	10.312051	-0.049890	4.815554
238.200938	7999.949114	10.317056	-0.049931	4.815586
238.181452	7999.882619	10.322061	-0.049927	4.815566
238.224741	7999.882275	10.327066	-0.049935	4.815566
238.100602	7999.865330	10.332071	-0.049912	4.815562
238.195921	7999.887186	10.337075	-0.049930	4.815567
238.118985	7999.864601	10.342080	-0.049916	4.815561
238.108185	7999.876191	10.347085	-0.049915	4.815565
238.312577	7999.888075	10.352090	-0.049953	4.815567
238.165291	7999.845128	10.357095	-0.049926	4.815555
238.187327	7999.854049	10.362099	-0.049930	4.815558
238.048990	7999.844347	10.367104	-0.049904	4.815556
238.093802	7999.850434	10.372109	-0.049913	4.815557
238.042056	7999.853884	10.377114	-0.049904	4.815558
238.042416	7999.903025	10.382119	-0.049904	4.815573
238.126433	7999.868108	10.387123	-0.049920	4.815562
238.012125	7999.856662	10.392128	-0.049899	4.815559
238.099066	7999.854892	10.397133	-0.049915	4.815558
238.241446	7999.904206	10.402138	-0.049942	4.815572
238.138459	7999.847031	10.407143	-0.049923	4.815556
238.111290	7999.857287	10.412147	-0.049918	4.815559
238.367252	7999.843316	10.417152	-0.049966	4.815554
238.099745	7999.881697	10.422157	-0.049917	4.815566
238.201562	7999.873763	10.427162	-0.049936	4.815563
238.218455	7999.862313	10.432167	-0.049939	4.815560
238.409674	7999.880389	10.437171	-0.049975	4.815564
238.324468	7999.952697	10.442176	-0.049959	4.815586
238.323888	7999.821379	10.447181	-0.049959	4.815547
238.417127	7999.876300	10.452186	-0.049977	4.815563
238.260631	7999.859897	10.457191	-0.049948	4.815559
238.245411	7999.869279	10.462195	-0.049945	4.815562
238.513847	7999.861918	10.467200	-0.049996	4.815558
238.325230	7999.883430	10.472205	-0.049961	4.815566
238.403836	7999.890066	10.477210	-0.049976	4.815567
238.386063	7999.850292	10.482215	-0.049973	4.815556
238.505046	7999.877872	10.487219	-0.049995	4.815563
238.244867	7999.843767	10.492224	-0.049947	4.815554
238.299608	7999.879912	10.497229	-0.049957	4.815565
238.504254	7999.908884	10.502234	-0.049996	4.815572
238.297588	7999.892732	10.507239	-0.049957	4.815568
238.155366	7999.900050	10.512243	-0.049931	4.815571
238.388630	7999.888914	10.517248	-0.049975	4.815567
238.400337	7999.884854	10.522253	-0.049977	4.815566
238.542702	7999.908543	10.527258	-0.050004	4.815572
238.164533	7999.879994	10.532263	-0.049934	4.815565
238.235542	7999.901455	10.537267	-0.049947	4.815571
238.385029	7999.881483	10.542272	-0.049975	4.815565
238.300152	7999.949525	10.547277	-0.049960	4.815585
238.393921	7999.875262	10.552282	-0.049977	4.815563
237.962381	7999.833034	10.557287	-0.049897	4.815552
237.975203	7999.854617	10.562291	-0.049900	4.815559
238.154308	7999.838329	10.567296	-0.049933	4.815553
238.345541	7999.859608	10.572301	-0.049969	4.815558
238.111619	7999.883587	10.577306	-0.049926	4.815567
238.228940	7999.854551	10.582311	-0.049948	4.815557
238.303613	7999.892087	10.587315	-0.049962	4.815568
238.212441	7999.887422	10.592320	-0.049945	4.815567
238.154561	7999.861944	10.597325	-0.049935	4.815560
238.188135	7999.882797	10.602330	-0.049941	4.815566
238.130933	7999.858398	10.607335	-0.049931	4.815559
238.114545	7999.894454	10.612339	-0.049928	4.815570
238.374261	7999.968098	10.617344	-0.049977	4.815590
238.369149	7999.866602	10.622349	-0.049976	4.815560
238.391795	7999.873396	10.627354	-0.049980	4.815562
238.229745	7999.827006	10.632359	-0.049950	4.815549
238.419449	7999.866412	10.637363	-0.049986	4.815560
238.343864	7999.854527	10.642368	-0.049972	4.815557
238.140356	7999.864052	10.647373	-0.049935	4.815561
238.165644	7999.871957	10.652378	-0.049939	4.815563
238.304783	7999.844343	10.657383	-0.049966	4.815554
238.232933	7999.843196	10.662387	-0.049952	4.815554
238.385852	7999.860650	10.667392	-0.049981	4.815558
238.412229	7999.968939	10.672397	-0.049986	4.815590
238.411369	7999.872850	10.677402	-0.049986	4.815562
238.370884	7999.855129	10.682407	-0.049979	4.815557
238.427144	7999.846454	10.687411	-0.049990	4.815554
238.380316	7999.882016	10.692416	-0.049981	4.815565
238.345354	7999.865452	10.697421	-0.049975	4.815560
238.755908	7999.897772	10.702426	-0.050052	4.815567
238.661865	7999.837538	10.707431	-0.050034	4.815550
238.518075	7999.858711	10.712435	-0.050008	4.815557
238.685754	7999.873202	10.717440	-0.050039	4.815561
238.744406	7999.869905	10.722445	-0.050051	4.815559
238.468374	7999.881454	10.727450	-0.049999	4.815564
238.435785	7999.853183	10.732455	-0.049993	4.815556
238.677283	7999.922261	10.737459	-0.050039	4.815575
238.602357	7999.886896	10.742464	-0.050025	4.815565
238.431502	7999.863852	10.747469	-0.049993	4.815559
238.395264	7999.882502	10.752474	-0.049987	4.815565
238.488828	7999.837064	10.757479	-0.050005	4.815551
238.435511	7999.930177	10.762483	-0.049995	4.815578
238.649416	7999.858934	10.767488	-0.050035	4.815557
238.732756	7999.860309	10.772493	-0.050051	4.815557
238.782254	7999.897437	10.777498	-0.050060	4.815567
238.585703	7999.857959	10.782503	-0.050024	4.815557
238.638071	7999.868440	10.787507	-0.050034	4.815559
238.737721	7999.880758	10.792512	-0.050053	4.815562
238.647106	7999.859018	10.797517	-0.050036	4.815557
238.732527	7999.894594	10.802522	-0.050052	4.815567
238.652256	7999.866617	10.807527	-0.050037	4.815559
238.639132	7999.890981	10.812531	-0.050035	4.815566
238.351050	7999.879912	10.817536	-0.049982	4.815564
238.550483	7999.856481	10.822541	-0.050019	4.815556
238.794425	7999.901041	10.827546	-0.050065	4.815568
238.297408	7999.860950	10.832551	-0.049972	4.815559
238.548643	7999.887476	10.837555	-0.050019	4.815565
238.721154	7999.876421	10.842560	-0.050052	4.815561
238.587168	7999.858247	10.847565	-0.050027	4.815557
238.462307	7999.905353	10.852570	-0.050004	4.815571
238.450182	7999.868873	10.857575	-0.050002	4.815560
238.724303	7999.884027	10.862579	-0.050053	4.815563
238.728577	7999.885185	10.867584	-0.050054	4.815564
238.754501	7999.846120	10.872589	-0.050059	4.815552
238.844417	7999.877499	10.877594	-0.050076	4.815561
238.691694	7999.958320	10.882599	-0.050048	4.815585
238.609686	7999.880130	10.887603	-0.050033	4.815563
238.604092	7999.878992	10.892608	-0.050032	4.815562
238.649959	7999.860538	10.897613	-0.050041	4.815557
238.610807	7999.888751	10.902618	-0.050034	4.815565
238.598008	7999.857599	10.907623	-0.050032	4.815556
238.637614	7999.853992	10.912627	-0.050039	4.815555
238.527180	7999.858624	10.917632	-0.050019	4.815557
238.499135	7999.864595	10.922637	-0.050014	4.815559
238.959070	7999.867821	10.927642	-0.050100	4.815557
238.844994	7999.835023	10.932647	-0.050079	4.815548
238.802941	7999.876001	10.937651	-0.050071	4.815561
238.986612	7999.977240	10.942656	-0.050106	4.815589
238.888815	7999.874234	10.947661	-0.050088	4.815560
238.878412	7999.907185	10.952666	-0.050086	4.815569
238.767701	7999.871238	10.957671	-0.050066	4.815559
238.988387	7999.898337	10.962675	-0.050107	4.815566
238.924872	7999.888783	10.967680	-0.050096	4.815564
238.695953	7999.897894	10.972685	-0.050053	4.815567
238.711885	7999.899241	10.977690	-0.050056	4.815568
238.664648	7999.849378	10.982695	-0.050048	4.815553
238.736402	7999.905019	10.987699	-0.050061	4.815569
238.961407	7999.895885	10.992704	-0.050103	4.815566
238.735146	7999.879413	10.997709	-0.050062	4.815562
238.792513	7999.891044	11.002714	-0.050073	4.815565
238.916215	7999.872788	11.007719	-0.050096	4.815559
238.945717	7999.904253	11.012723	-0.050102	4.815568
238.857797	7999.853728	11.017728	-0.050085	4.815554
238.847730	7999.865329	11.022733	-0.050084	4.815557
239.113554	7999.908110	11.027738	-0.050133	4.815568
238.881039	7999.881928	11.032743	-0.050090	4.815562
238.682632	7999.878722	11.037747	-0.050054	4.815562
238.872758	7999.887172	11.042752	-0.050089	4.815563
238.933120	7999.904190	11.047757	-0.050101	4.815568
238.753792	7999.914107	11.052762	-0.050068	4.815572
238.699175	7999.891885	11.057767	-0.050058	4.815566
238.722716	7999.920049	11.062771	-0.050062	4.815574
238.907033	7999.903847	11.067776	-0.050097	4.815568
238.648254	7999.911405	11.072781	-0.050049	4.815572
238.784766	7999.915780	11.077786	-0.050075	4.815572
238.763738	7999.967778	11.082791	-0.050071	4.815587
238.696854	7999.910121	11.087795	-0.050059	4.815571
238.932364	7999.916106	11.092800	-0.050103	4.815572
238.898821	7999.891023	11.097805	-0.050097	4.815564
238.881083	7999.908906	11.102810	-0.050094	4.815570
238.898901	7999.910284	11.107815	-0.050097	4.815570
239.172654	7999.903010	11.112819	-0.050148	4.815567
238.965273	7999.911404	11.117824	-0.050110	4.815570
238.985138	7999.889325	11.122829	-0.050114	4.815563
239.079275	7999.919705	11.127834	-0.050132	4.815572
238.947476	7999.890888	11.132839	-0.050107	4.815564
238.882306	7999.904797	11.137843	-0.050096	4.815568
239.028241	7999.903987	11.142848	-0.050123	4.815567
238.920023	7999.896909	11.147853	-0.050103	4.815566
238.979973	7999.904311	11.152858	-0.050114	4.815568
238.940884	7999.884476	11.157863	-0.050107	4.815562
238.878846	7999.871743	11.162867	-0.050096	4.815559
239.124723	7999.880032	11.167872	-0.050142	4.815560
239.037364	7999.848735	11.172877	-0.050126	4.815551
239.223366	7999.875270	11.177882	-0.050161	4.815558
239.182193	7999.889569	11.182887	-0.050153	4.815562
238.998329	7999.885532	11.187891	-0.050119	4.815562
239.092290	7999.921248	11.192896	-0.050137	4.815572
239.053571	7999.892877	11.197901	-0.050130	4.815564
239.071891	7999.930567	11.202906	-0.050134	4.815575
239.107276	7999.890588	11.207911	-0.050141	4.815563
239.311076	7999.906736	11.212915	-0.050179	4.815567
239.154255	7999.915951	11.217920	-0.050150	4.815570
238.770011	7999.901181	11.222925	-0.050079	4.815568
239.106507	7999.917351	11.227930	-0.050141	4.815571
239.153777	7999.864752	11.232935	-0.050150	4.815555
238.826126	7999.878664	11.237939	-0.050090	4.815561
238.886615	7999.896752	11.242944	-0.050101	4.815566
238.870774	7999.874092	11.247949	-0.050098	4.815559
239.125318	7999.898539	11.252954	-0.050146	4.815565
238.852856	7999.870638	11.257959	-0.050096	4.815558
239.112213	7999.904773	11.262963	-0.050144	4.815567
239.238524	7999.904712	11.267968	-0.050168	4.815567
238.850717	7999.889884	11.272973	-0.050096	4.815564
239.032973	7999.923832	11.277978	-0.050130	4.815573
238.978922	7999.897348	11.282983	-0.050120	4.815566
238.952220	7999.893731	11.287987	-0.050116	4.815565
239.230076	7999.979418	11.292992	-0.050168	4.815588
239.175541	7999.866438	11.297997	-0.050158	4.815556
239.281171	7999.876718	11.303002	-0.050177	4.815558
238.937888	7999.858344	11.308007	-0.050114	4.815554
239.139301	7999.897942	11.313011	-0.050152	4.815565
239.308380	7999.916728	11.318016	-0.050183	4.815570
239.114236	7999.893304	11.323021	-0.050147	4.815564
238.887405	7999.897110	11.328026	-0.050105	4.815566
239.111830	7999.874086	11.333031	-0.050147	4.815558
239.222632	7999.873773	11.338035	-0.050168	4.815557
238.944306	7999.904503	11.343040	-0.050117	4.815568
238.902631	7999.912387	11.348045	-0.050109	4.815570
239.112708	7999.916892	11.353050	-0.050148	4.815571
239.117787	7999.912724	11.358055	-0.050150	4.815569
239.177808	7999.899839	11.363059	-0.050161	4.815565
239.442729	7999.908439	11.368064	-0.050211	4.815567
239.061480	7999.884108	11.373069	-0.050140	4.815561
239.167884	7999.920026	11.378074	-0.050160	4.815571
239.194946	7999.907673	11.383079	-0.050165	4.815567
239.016733	7999.913338	11.388083	-0.050132	4.815570
239.080156	7999.909051	11.393088	-0.050144	4.815568
239.029787	7999.855932	11.398093	-0.050135	4.815553
239.058339	7999.904466	11.403098	-0.050141	4.815567
239.008520	7999.896202	11.408103	-0.050132	4.815565
239.252174	7999.925810	11.413107	-0.050177	4.815572
239.190638	7999.912017	11.418112	-0.050166	4.815569
239.037863	7999.977888	11.423117	-0.050138	4.815589
239.125600	7999.890712	11.428122	-0.050154	4.815563
239.272841	7999.861095	11.433127	-0.050182	4.815553
239.210385	7999.870777	11.438131	-0.050171	4.815557
239.191965	7999.896124	11.443136	-0.050167	4.815564
239.174799	7999.870239	11.448141	-0.050164	4.815557
239.324342	7999.894046	11.453146	-0.050192	4.815563
239.160276	7999.847621	11.458151	-0.050162	4.815550
238.986314	7999.888590	11.463155	-0.050130	4.815563
239.134271	7999.879271	11.468160	-0.050158	4.815559
238.958123	7999.871088	11.473165	-0.050125	4.815558
239.046912	7999.872552	11.478170	-0.050142	4.815558
238.992716	7999.940027	11.483175	-0.050132	4.815578
239.217376	7999.849739	11.488179	-0.050174	4.815550
239.134101	7999.879370	11.493184	-0.050159	4.815559
239.046555	7999.856611	11.498189	-0.050143	4.815553
239.310848	7999.895098	11.503194	-0.050192	4.815563
239.350686	7999.892562	11.508199	-0.050200	4.815562
239.341132	7999.899902	11.513203	-0.050198	4.815564
239.288518	7999.896931	11.518208	-0.050189	4.815564
239.185576	7999.886735	11.523213	-0.050170	4.815561
239.201542	7999.908370	11.528218	-0.050173	4.815567
239.324570	7999.865546	11.533223	-0.050196	4.815554
239.376837	7999.882432	11.538227	-0.050206	4.815559
239.354889	7999.905586	11.543232	-0.050202	4.815566
239.113406	7999.858969	11.548237	-0.050158	4.815553
239.389735	7999.894448	11.553242	-0.050209	4.815562
239.312283	7999.974358	11.558247	-0.050195	4.815586
239.161363	7999.899317	11.563251	-0.050167	4.815565
239.298493	7999.891958	11.568256	-0.050193	4.815562
239.219061	7999.886415	11.573261	-0.050178	4.815561
239.304497	7999.925196	11.578266	-0.050195	4.815572
239.349945	7999.899262	11.583271	-0.050203	4.815564
239.302649	7999.881429	11.588275	-0.050195	4.815559
239.372673	7999.899672	11.593280	-0.050208	4.815564
239.379919	7999.845355	11.598285	-0.050210	4.815548
239.511697	7999.922261	11.603290	-0.050234	4.815570
239.461676	7999.889435	11.608295	-0.050225	4.815561
239.211632	7999.901405	11.613299	-0.050179	4.815565
239.198639	7999.910824	11.618304	-0.050177	4.815568
239.191001	7999.887230	11.623309	-0.050176	4.815561
239.309800	7999.907334	11.628314	-0.050198	4.815567
239.431766	7999.891186	11.633319	-0.050221	4.815561
239.491188	7999.899647	11.638323	-0.050232	4.815563
239.466863	7999.905678	11.643328	-0.050228	4.815565
239.342668	7999.897272	11.648333	-0.050205	4.815563
239.276615	7999.923980	11.653338	-0.050193	4.815572
239.140597	7999.880146	11.658343	-0.050168	4.815559
239.002361	7999.901409	11.663347	-0.050142	4.815566
239.402735	7999.900466	11.668352	-0.050217	4.815564
239.502400	7999.901039	11.673357	-0.050236	4.815564
239.354265	7999.913599	11.678362	-0.050209	4.815568
239.225354	7999.890168	11.683367	-0.050185	4.815562
239.210890	7999.885682	11.688371	-0.050182	4.815561
239.427213	7999.902033	11.693376	-0.050223	4.815564
239.393097	7999.868398	11.698381	-0.050217	4.815555
239.482646	7999.907247	11.703386	-0.050234	4.815566
239.334616	7999.874962	11.708391	-0.050206	4.815557
239.429194	7999.898944	11.713395	-0.050224	4.815563
239.316111	7999.904599	11.718400	-0.050203	4.815566
239.177013	7999.879934	11.723405	-0.050178	4.815559
239.305906	7999.905541	11.728410	-0.050202	4.815566
239.162288	7999.870126	11.733415	-0.050175	4.815556
239.296248	7999.974829	11.738419	-0.050201	4.815586
239.313781	7999.900392	11.743424	-0.050204	4.815564
239.167805	7999.887360	11.748429	-0.050177	4.815561
239.277462	7999.914790	11.753434	-0.050198	4.815569
239.218883	7999.872216	11.758439	-0.050187	4.815557
239.227266	7999.896930	11.763443	-0.050189	4.815564
239.164585	7999.866034	11.768448	-0.050177	4.815555
239.299537	7999.882130	11.773453	-0.050203	4.815559
239.468166	7999.916926	11.778458	-0.050234	4.815568
239.316236	7999.883510	11.783463	-0.050206	4.815559
239.252481	7999.897442	11.788467	-0.050195	4.815564
239.436679	7999.878035	11.793472	-0.050229	4.815557
239.319935	7999.874021	11.798477	-0.050208	4.815557
239.436751	7999.884484	11.803482	-0.050230	4.815559
239.212401	7999.868042	11.808487	-0.050188	4.815555
239.131641	7999.890240	11.813491	-0.050173	4.815562
239.406776	7999.900073	11.818496	-0.050225	4.815564
239.353203	7999.871461	11.823501	-0.050215	4.815556
239.505374	7999.915599	11.828506	-0.050244	4.815568
239.426421	7999.892980	11.833511	-0.050229	4.815562
239.475593	7999.903410	11.838515	-0.050239	4.815564
239.554491	7999.916458	11.843520	-0.050253	4.815568
239.360941	7999.872756	11.848525	-0.050218	4.815556
239.453870	7999.926608	11.853530	-0.050235	4.815571
239.461112	7999.963050	11.858535	-0.050237	4.815582
239.236818	7999.893221	11.863539	-0.050195	4.815562
239.328317	7999.913949	11.868544	-0.050213	4.815568
239.314182	7999.875300	11.873549	-0.050210	4.815557
239.512669	7999.920192	11.878554	-0.050247	4.815569
239.312858	7999.876387	11.883559	-0.050210	4.815557
239.280435	7999.905777	11.888563	-0.050205	4.815566
239.371892	7999.915827	11.893568	-0.050222	4.815568
239.199042	7999.871394	11.898573	-0.050190	4.815556
239.436580	7999.889158	11.903578	-0.050234	4.815560
239.410923	7999.879152	11.908583	-0.050230	4.815557
239.151893	7999.883501	11.913587	-0.050182	4.815560
239.327801	7999.897060	11.918592	-0.050215	4.815563
239.372112	7999.889259	11.923597	-0.050223	4.815561
239.465523	7999.910018	11.928602	-0.050241	4.815566
239.196818	7999.901397	11.933607	-0.050191	4.815565
239.407557	7999.888829	11.938611	-0.050231	4.815560
239.470999	7999.909100	11.943616	-0.050243	4.815566
239.402150	7999.873833	11.948621	-0.050230	4.815556
239.378851	7999.908710	11.953626	-0.050226	4.815566
239.689235	7999.892424	11.958631	-0.050284	4.815560
239.530475	7999.909081	11.963635	-0.050255	4.815566
239.360765	7999.903138	11.968640	-0.050223	4.815565
239.315789	7999.858649	11.973645	-0.050215	4.815552
239.508853	7999.918400	11.978650	-0.050251	4.815568
239.170057	7999.905436	11.983655	-0.050188	4.815566
239.352451	7999.899881	11.988659	-0.050223	4.815564
239.374218	7999.910933	11.993664	-0.050227	4.815567
239.278023	7999.896575	11.998669	-0.050209	4.815563
239.443015	7999.922770	12.003674	-0.050240	4.815570
239.564745	7999.891670	12.008679	-0.050263	4.815560
239.530850	7999.907155	12.013683	-0.050257	4.815565
239.616529	7999.921382	12.018688	-0.050273	4.815569
239.453383	7999.873903	12.023693	-0.050243	4.815556
239.508925	7999.928215	12.028698	-0.050254	4.815571
239.326479	7999.908183	12.033703	-0.050220	4.815566
239.485428	7999.976990	12.038707	-0.050250	4.815586
239.616060	7999.909731	12.043712	-0.050274	4.815565
239.560751	7999.860802	12.048717	-0.050264	4.815551
239.443611	7999.910170	12.053722	-0.050243	4.815566
239.507011	7999.882392	12.058727	-0.050255	4.815558
239.462979	7999.890238	12.063731	-0.050247	4.815560
239.504591	7999.919765	12.068736	-0.050255	4.815569
239.371264	7999.870635	12.073741	-0.050230	4.815555
239.532843	7999.913858	12.078746	-0.050260	4.815567
239.588954	7999.910520	12.083751	-0.050271	4.815566
239.408421	7999.912943	12.088755	-0.050238	4.815567
239.707611	7999.935982	12.093760	-0.050294	4.815572
239.703502	7999.884683	12.098765	-0.050293	4.815557
239.545375	7999.930180	12.103770	-0.050264	4.815572
239.528542	7999.898962	12.108775	-0.050261	4.815562
239.489001	7999.918626	12.113779	-0.050254	4.815568
239.520864	7999.926639	12.118784	-0.050260	4.815571
239.444773	7999.864560	12.123789	-0.050246	4.815553
239.504503	7999.934956	12.128794	-0.050257	4.815573
239.367449	7999.895375	12.133799	-0.050232	4.815562
239.192069	7999.900018	12.138803	-0.050200	4.815564
239.559993	7999.903887	12.143808	-0.050268	4.815564
239.319517	7999.869031	12.148813	-0.050224	4.815555
239.276387	7999.881163	12.153818	-0.050216	4.815558
239.522611	7999.879849	12.158823	-0.050262	4.815557
239.416934	7999.917657	12.163827	-0.050243	4.815568
239.379188	7999.880760	12.168832	-0.050236	4.815558
239.437173	7999.865707	12.173837	-0.050247	4.815553
239.564577	7999.920120	12.178842	-0.050271	4.815568
239.505395	7999.885009	12.183847	-0.050260	4.815558
239.376039	7999.928839	12.188851	-0.050236	4.815572
239.504999	7999.935228	12.193856	-0.050261	4.815573
239.521051	7999.909883	12.198861	-0.050264	4.815566
239.433363	7999.935171	12.203866	-0.050248	4.815573
239.507298	7999.913971	12.208871	-0.050262	4.815567
239.416740	7999.913586	12.213875	-0.050245	4.815567
239.429075	7999.924485	12.218880	-0.050248	4.815570
239.327959	7999.864134	12.223885	-0.050229	4.815553
239.552542	7999.908382	12.228890	-0.050271	4.815565
239.531237	7999.897378	12.233895	-0.050267	4.815562
239.262555	7999.852454	12.238899	-0.050217	4.815550
239.411567	7999.878388	12.243904	-0.050245	4.815557
239.553494	7999.892462	12.248909	-0.050272	4.815560
239.453108	7999.915408	12.253914	-0.050254	4.815567
239.453476	7999.880198	12.258919	-0.050254	4.815557
239.810165	7999.882817	12.263923	-0.050321	4.815556
239.831998	7999.867176	12.268928	-0.050325	4.815552
239.670338	7999.866703	12.273933	-0.050295	4.815552
239.726512	7999.942380	12.278938	-0.050306	4.815574
239.788771	7999.874009	12.283943	-0.050318	4.815554
239.487253	7999.891547	12.288947	-0.050262	4.815560
239.365865	7999.882119	12.293952	-0.050239	4.815558
239.489657	7999.883085	12.298957	-0.050263	4.815558
239.520473	7999.913504	12.303962	-0.050269	4.815567
239.340662	7999.896719	12.308967	-0.050235	4.815562
239.680529	7999.900132	12.313971	-0.050299	4.815562
239.662562	7999.915876	12.318976	-0.050296	4.815567
239.654003	7999.870911	12.323981	-0.050294	4.815553
239.659355	7999.893442	12.328986	-0.050296	4.815560
239.701447	7999.890943	12.333991	-0.050304	4.815559
239.494776	7999.883331	12.338995	-0.050265	4.815558
239.654712	7999.901969	12.344000	-0.050295	4.815562
239.507648	7999.893191	12.349005	-0.050268	4.815561
239.452058	7999.916865	12.354010	-0.050258	4.815568
239.508210	7999.871885	12.359015	-0.050269	4.815554
239.617773	7999.918534	12.364019	-0.050289	4.815567
239.628829	7999.950767	12.369024	-0.050292	4.815577
239.546488	7999.885382	12.374029	-0.050277	4.815558
239.699774	7999.895370	12.379034	-0.050305	4.815560
239.792261	7999.880879	12.384039	-0.050323	4.815556
239.761207	7999.893207	12.389043	-0.050317	4.815559
239.736683	7999.918455	12.394048	-0.050313	4.815567
239.699357	7999.844192	12.399053	-0.050306	4.815545
239.639628	7999.890222	12.404058	-0.050295	4.815559
239.693190	7999.888978	12.409063	-0.050306	4.815558
239.622040	7999.875028	12.414067	-0.050293	4.815555
239.622430	7999.990374	12.419072	-0.050293	4.815588
239.490750	7999.890018	12.424077	-0.050269	4.815560
239.636491	7999.907357	12.429082	-0.050296	4.815564
239.748400	7999.882504	12.434087	-0.050317	4.815556
239.638565	7999.910635	12.439091	-0.050297	4.815565
239.791473	7999.901397	12.444096	-0.050326	4.815562
239.862343	7999.857724	12.449101	-0.050339	4.815548
239.689751	7999.904054	12.454106	-0.050307	4.815563
239.679273	7999.891091	12.459111	-0.050305	4.815559
239.848527	7999.897068	12.464115	-0.050337	4.815560
239.677111	7999.914587	12.469120	-0.050305	4.815566
239.604576	7999.877124	12.474125	-0.050292	4.815555
239.655159	7999.896119	12.479130	-0.050302	4.815561
239.844862	7999.890683	12.484135	-0.050337	4.815558
239.764292	7999.888325	12.489139	-0.050323	4.815558
239.882552	7999.912692	12.494144	-0.050345	4.815564
239.690448	7999.897842	12.499149	-0.050309	4.815561
239.860997	7999.900637	12.504154	-0.050341	4.815561
239.744904	7999.890226	12.509159	-0.050320	4.815558
239.571759	7999.877820	12.514163	-0.050288	4.815556
239.811883	7999.927661	12.519168	-0.050333	4.815569
239.795694	7999.892181	12.524173	-0.050330	4.815559
239.697483	7999.937586	12.529178	-0.050312	4.815572
239.790246	7999.918827	12.534183	-0.050329	4.815567
239.705462	7999.900384	12.539187	-0.050314	4.815562
239.756255	7999.911909	12.544192	-0.050324	4.815565
239.660715	7999.897561	12.549197	-0.050306	4.815561
239.688421	7999.925794	12.554202	-0.050311	4.815569
239.767004	7999.886518	12.559207	-0.050326	4.815557
239.691883	7999.914146	12.564211	-0.050313	4.815566
239.737694	7999.911708	12.569216	-0.050321	4.815565
239.649011	7999.877185	12.574221	-0.050305	4.815555
239.792540	7999.912641	12.579226	-0.050332	4.815565
239.888927	7999.974025	12.584231	-0.050350	4.815582
239.971364	7999.873948	12.589235	-0.050366	4.815552
240.050240	7999.915827	12.594240	-0.050381	4.815564
239.931419	7999.884016	12.599245	-0.050359	4.815556
239.927838	7999.921351	12.604250	-0.050358	4.815567
239.769374	7999.891031	12.609255	-0.050329	4.815558
239.872137	7999.859622	12.614259	-0.050348	4.815549
240.021635	7999.903718	12.619264	-0.050377	4.815561
239.972161	7999.916814	12.624269	-0.050368	4.815565
239.935123	7999.947197	12.629274	-0.050361	4.815574
239.850755	7999.892456	12.634279	-0.050345	4.815558
239.760795	7999.923046	12.639283	-0.050329	4.815568
239.810521	7999.924943	12.644288	-0.050338	4.815568
239.947767	7999.899435	12.649293	-0.050364	4.815560
240.096876	7999.942456	12.654298	-0.050392	4.815572
239.868122	7999.919535	12.659303	-0.050350	4.815566
239.838718	7999.901992	12.664307	-0.050345	4.815561
239.986776	7999.931116	12.669312	-0.050372	4.815569
239.923383	7999.893801	12.674317	-0.050361	4.815558
240.009497	7999.926187	12.679322	-0.050377	4.815567
240.119715	7999.913052	12.684327	-0.050398	4.815563
240.025481	7999.907268	12.689331	-0.050381	4.815562
240.178501	7999.903372	12.694336	-0.050409	4.815560
240.105165	7999.907538	12.699341	-0.050396	4.815562
239.993564	7999.931369	12.704346	-0.050375	4.815569
240.015016	7999.927467	12.709351	-0.050379	4.815568
239.873606	7999.919848	12.714355	-0.050353	4.815566
239.954240	7999.923316	12.719360	-0.050369	4.815567
240.057325	7999.897251	12.724365	-0.050388	4.815559
240.070274	7999.912431	12.729370	-0.050391	4.815563
240.025059	7999.921325	12.734375	-0.050383	4.815566
239.855622	7999.949554	12.739379	-0.050351	4.815575
240.121947	7999.938959	12.744384	-0.050401	4.815571
240.200111	7999.914625	12.749389	-0.050416	4.815563
240.168511	7999.933351	12.754394	-0.050410	4.815569
240.233722	7999.904534	12.759399	-0.050423	4.815560
240.108551	7999.928145	12.764403	-0.050399	4.815567
240.183497	7999.925113	12.769408	-0.050414	4.815566
240.136930	7999.915834	12.774413	-0.050405	4.815564
240.047993	7999.938966	12.779418	-0.050389	4.815571
239.913686	7999.915446	12.784423	-0.050364	4.815565
240.052024	7999.877141	12.789427	-0.050390	4.815553
240.087982	7999.927932	12.794432	-0.050397	4.815567
239.919806	7999.910267	12.799437	-0.050366	4.815563
239.825015	7999.906610	12.804442	-0.050349	4.815562
239.969532	7999.914320	12.809447	-0.050376	4.815564
239.826790	7999.920560	12.814451	-0.050349	4.815567
240.025998	7999.916347	12.819456	-0.050387	4.815564
240.011179	7999.908652	12.824461	-0.050384	4.815562
239.928847	7999.953247	12.829466	-0.050369	4.815576
239.904791	7999.934724	12.834471	-0.050365	4.815570
240.017969	7999.914163	12.839475	-0.050386	4.815564
240.045633	7999.939192	12.844480	-0.050391	4.815571
239.904537	7999.909154	12.849485	-0.050365	4.815563
239.955416	7999.903596	12.854490	-0.050375	4.815561
240.085109	7999.902523	12.859495	-0.050400	4.815560
240.035617	7999.913484	12.864499	-0.050391	4.815563
240.060500	7999.932061	12.869504	-0.050395	4.815569
239.985361	7999.890283	12.874509	-0.050382	4.815557
239.856151	7999.907421	12.879514	-0.050358	4.815562
239.915105	7999.914807	12.884519	-0.050369	4.815564
240.084914	7999.986997	12.889523	-0.050401	4.815585
239.897158	7999.942318	12.894528	-0.050366	4.815572
239.583335	7999.912674	12.899533	-0.050308	4.815565
239.763776	7999.941257	12.904538	-0.050342	4.815573
240.103148	7999.883800	12.909543	-0.050405	4.815554
239.924270	7999.907604	12.914547	-0.050372	4.815562
240.071186	7999.926032	12.919552	-0.050400	4.815567
239.999774	7999.927025	12.924557	-0.050387	4.815567
240.167254	7999.930839	12.929562	-0.050418	4.815568
239.975733	7999.943759	12.934567	-0.050383	4.815572
240.068373	7999.922864	12.939571	-0.050400	4.815566
240.142193	7999.964661	12.944576	-0.050414	4.815578
239.866329	7999.920685	12.949581	-0.050363	4.815566
240.091716	7999.937186	12.954586	-0.050405	4.815570
240.243486	7999.901235	12.959591	-0.050434	4.815559
240.060468	7999.932447	12.964595	-0.050400	4.815569
239.941430	7999.925191	12.969600	-0.050378	4.815567
239.984397	7999.882132	12.974605	-0.050386	4.815554
240.110756	7999.935462	12.979610	-0.050410	4.815569
240.114573	7999.924866	12.984615	-0.050411	4.815566
239.976760	7999.907695	12.989619	-0.050385	4.815562
240.087277	7999.928734	12.994624	-0.050406	4.815567
240.116431	7999.902534	12.999629	-0.050412	4.815560
240.019990	7999.891375	13.004634	-0.050394	4.815557
240.199888	7999.925288	13.009639	-0.050428	4.815566
240.074267	7999.927536	13.014643	-0.050405	4.815567
240.266563	7999.922143	13.019648	-0.050441	4.815565
240.144774	7999.884945	13.024653	-0.050418	4.815554
240.112422	7999.901523	13.029658	-0.050413	4.815559
240.149450	7999.901078	13.034663	-0.050420	4.815559
240.027324	7999.877756	13.039667	-0.050397	4.815553
239.931156	7999.953091	13.044672	-0.050379	4.815575
240.078933	7999.912805	13.049677	-0.050407	4.815563
239.991384	7999.935960	13.054682	-0.050391	4.815570
240.263576	7999.895562	13.059687	-0.050442	4.815557
240.135714	7999.879621	13.064691	-0.050418	4.815553
240.055032	7999.924243	13.069696	-0.050404	4.815566
240.083351	7999.896962	13.074701	-0.050409	4.815558
240.070212	7999.910650	13.079706	-0.050407	4.815562
239.971832	7999.906934	13.084711	-0.050389	4.815562
240.088165	7999.913118	13.089715	-0.050411	4.815563
240.326546	7999.944780	13.094720	-0.050455	4.815571
240.192314	7999.914853	13.099725	-0.050431	4.815563
239.970027	7999.945426	13.104730	-0.050390	4.815573
240.145029	7999.918396	13.109735	-0.050422	4.815564
240.192678	7999.929869	13.114739	-0.050431	4.815567
239.974144	7999.935944	13.119744	-0.050391	4.815570
239.961435	7999.886639	13.124749	-0.050389	4.815556
239.886884	7999.901463	13.129754	-0.050375	4.815560
240.009635	7999.907752	13.134759	-0.050398	4.815562
239.793631	7999.902122	13.139763	-0.050358	4.815561
240.026836	7999.923021	13.144768	-0.050402	4.815566
240.082669	7999.923950	13.149773	-0.050413	4.815566
240.143608	7999.963402	13.154778	-0.050424	4.815577
240.264656	7999.954715	13.159783	-0.050447	4.815574
239.872213	7999.894960	13.164787	-0.050374	4.815558
240.028627	7999.939169	13.169792	-0.050403	4.815571
240.119007	7999.920372	13.174797	-0.050420	4.815565
240.218383	7999.950840	13.179802	-0.050439	4.815573
240.203114	7999.936730	13.184807	-0.050437	4.815569
240.074137	7999.910093	13.189811	-0.050413	4.815562
240.182996	7999.933240	13.194816	-0.050433	4.815568
239.983470	7999.905455	13.199821	-0.050396	4.815561
239.932028	7999.927062	13.204826	-0.050387	4.815567
240.093195	7999.923298	13.209831	-0.050417	4.815566
239.967218	7999.907387	13.214835	-0.050394	4.815562
240.225078	7999.942569	13.219840	-0.050442	4.815571
240.071561	7999.905922	13.224845	-0.050414	4.815561
240.163273	7999.933062	13.229850	-0.050431	4.815568
240.194863	7999.936799	13.234855	-0.050437	4.815569
239.992785	7999.919650	13.239859	-0.050400	4.815565
240.160494	7999.940552	13.244864	-0.050431	4.815570
240.019379	7999.923327	13.249869	-0.050405	4.815566
239.905993	7999.940723	13.254874	-0.050385	4.815572
240.370938	7999.941902	13.259879	-0.050471	4.815570
240.179260	7999.939871	13.264883	-0.050436	4.815570
240.065117	7999.933763	13.269888	-0.050415	4.815569
240.130920	7999.915634	13.274893	-0.050427	4.815563
240.351030	7999.935253	13.279898	-0.050469	4.815568
240.122396	7999.937959	13.284903	-0.050426	4.815570
239.968183	7999.920521	13.289907	-0.050398	4.815565
240.082043	7999.929869	13.294912	-0.050419	4.815567
240.017056	7999.891459	13.299917	-0.050407	4.815557
239.994501	7999.923146	13.304922	-0.050403	4.815566
240.222646	7999.922608	13.309927	-0.050446	4.815565
240.180660	7999.914470	13.314931	-0.050438	4.815562
240.249001	7999.964721	13.319936	-0.050451	4.815577
240.163540	7999.937723	13.324941	-0.050436	4.815569
240.281037	7999.948198	13.329946	-0.050458	4.815572
240.194262	7999.952145	13.334951	-0.050442	4.815573
240.202051	7999.914920	13.339955	-0.050444	4.815562
240.323878	7999.930804	13.344960	-0.050467	4.815567
240.233929	7999.905869	13.349965	-0.050450	4.815560
240.145748	7999.945030	13.354970	-0.050434	4.815572
240.112669	7999.937038	13.359975	-0.050428	4.815569
239.976236	7999.914550	13.364979	-0.050403	4.815563
239.951181	7999.941925	13.369984	-0.050398	4.815572
239.986678	7999.899812	13.374989	-0.050405	4.815559
240.072724	7999.951418	13.379994	-0.050421	4.815574
240.291801	7999.944326	13.384999	-0.050462	4.815571
240.180611	7999.932927	13.390003	-0.050442	4.815568
240.157446	7999.929367	13.395008	-0.050438	4.815567
240.154007	7999.918653	13.400013	-0.050437	4.815564
240.112740	7999.922273	13.405018	-0.050430	4.815565
240.328479	7999.918330	13.410023	-0.050470	4.815563
240.238804	7999.927569	13.415027	-0.050454	4.815566
240.304742	7999.938272	13.420032	-0.050466	4.815569
240.220242	7999.898477	13.425037	-0.050451	4.815557
240.192819	7999.914068	13.430042	-0.050446	4.815562
240.298471	7999.925418	13.435047	-0.050466	4.815565
240.115861	7999.877619	13.440051	-0.050432	4.815552
240.100472	7999.912626	13.445056	-0.050430	4.815562
240.043296	7999.888225	13.450061	-0.050419	4.815555
239.991674	7999.908761	13.455066	-0.050410	4.815562
240.089857	7999.913582	13.460071	-0.050428	4.815562
240.138078	7999.926133	13.465075	-0.050438	4.815566
240.108933	7999.939560	13.470080	-0.050432	4.815570
240.130759	7999.911105	13.475085	-0.050437	4.815562
240.137847	7999.961427	13.480090	-0.050438	4.815576
240.086423	7999.925374	13.485095	-0.050429	4.815566
240.030958	7999.928763	13.490099	-0.050419	4.815567
240.277006	7999.947736	13.495104	-0.050465	4.815572
240.272976	7999.918860	13.500109	-0.050464	4.815563
240.145529	7999.889044	13.505114	-0.050441	4.815555
240.168220	7999.920400	13.510119	-0.050445	4.815564
240.175690	7999.884237	13.515123	-0.050447	4.815553
240.387436	7999.920804	13.520128	-0.050487	4.815563
240.118260	7999.964495	13.525133	-0.050437	4.815577
240.170411	7999.932262	13.530138	-0.050447	4.815567
240.190672	7999.916596	13.535143	-0.050451	4.815563
240.084725	7999.881791	13.540147	-0.050431	4.815553
240.336118	7999.938223	13.545152	-0.050478	4.815568
240.310711	7999.909000	13.550157	-0.050474	4.815560
240.219820	7999.876575	13.555162	-0.050457	4.815551
240.227732	7999.901283	13.560167	-0.050459	4.815558
240.038090	7999.886472	13.565171	-0.050424	4.815555
240.152877	7999.937479	13.570176	-0.050445	4.815569
240.178120	7999.898402	13.575181	-0.050450	4.815557
240.059928	7999.903973	13.580186	-0.050428	4.815560
240.461803	7999.915872	13.585191	-0.050503	4.815561
240.131192	7999.907309	13.590195	-0.050442	4.815560
240.327223	7999.927604	13.595200	-0.050479	4.815565
240.370808	7999.917656	13.600205	-0.050487	4.815562
240.266563	7999.897827	13.605210	-0.050468	4.815557
240.281186	7999.906628	13.610215	-0.050471	4.815559
240.304973	7999.901696	13.615219	-0.050476	4.815558
240.406613	7999.951421	13.620224	-0.050495	4.815572
240.204823	7999.911853	13.625229	-0.050457	4.815561
240.244198	7999.929599	13.630234	-0.050465	4.815566
240.194503	7999.915997	13.635239	-0.050456	4.815562
240.158209	7999.905816	13.640243	-0.050449	4.815560
240.208788	7999.933354	13.645248	-0.050459	4.815567
240.329560	7999.928934	13.650253	-0.050482	4.815566
240.289389	7999.956063	13.655258	-0.050475	4.815574
240.312084	7999.934029	13.660263	-0.050479	4.815567
240.032414	7999.914549	13.665267	-0.050427	4.815563
240.248580	7999.930900	13.670272	-0.050468	4.815567
240.041060	7999.911527	13.675277	-0.050429	4.815562
239.979487	7999.915884	13.680282	-0.050418	4.815563
240.207587	7999.920684	13.685287	-0.050461	4.815564
240.140542	7999.908936	13.690291	-0.050448	4.815561
240.129282	7999.909840	13.695296	-0.050447	4.815561
240.100518	7999.866681	13.700301	-0.050441	4.815548
240.118055	7999.895817	13.705306	-0.050445	4.815557
240.197451	7999.923824	13.710311	-0.050460	4.815565
239.953813	7999.901728	13.715315	-0.050415	4.815559
240.177467	7999.911794	13.720320	-0.050457	4.815561
240.053650	7999.900189	13.725325	-0.050434	4.815558
240.157446	7999.902967	13.730330	-0.050453	4.815559
240.117171	7999.900196	13.735335	-0.050446	4.815558
240.131441	7999.897245	13.740339	-0.050449	4.815557
240.311597	7999.924756	13.745344	-0.050483	4.815564
240.173518	7999.893699	13.750349	-0.050457	4.815556
240.263123	7999.894110	13.755354	-0.050474	4.815556
240.405073	7999.901779	13.760359	-0.050501	4.815557
240.292105	7999.889283	13.765363	-0.050480	4.815554
240.413498	7999.939330	13.770368	-0.050503	4.815568
240.268458	7999.906024	13.775373	-0.050476	4.815559
240.207899	7999.987279	13.780378	-0.050465	4.815583
240.515124	7999.930367	13.785383	-0.050523	4.815565
240.334355	7999.910361	13.790387	-0.050489	4.815560
240.277872	7999.935089	13.795392	-0.050479	4.815567
240.196594	7999.910295	13.800397	-0.050464	4.815561
240.385100	7999.902705	13.805402	-0.050499	4.815557
240.220146	7999.907516	13.810407	-0.050469	4.815560
240.052835	7999.912288	13.815411	-0.050438	4.815562
240.337075	7999.940425	13.820416	-0.050491	4.815569
240.305972	7999.921787	13.825421	-0.050486	4.815563
240.203831	7999.914806	13.830426	-0.050467	4.815562
240.404683	7999.942654	13.835431	-0.050504	4.815569
240.264991	7999.915842	13.840435	-0.050479	4.815562
240.217724	7999.934313	13.845440	-0.050470	4.815567
240.347246	7999.900137	13.850445	-0.050494	4.815557
240.371856	7999.921913	13.855450	-0.050499	4.815563
240.374215	7999.939057	13.860455	-0.050500	4.815568
240.310605	7999.933771	13.865459	-0.050488	4.815567
240.407542	7999.965267	13.870464	-0.050507	4.815576
240.434629	7999.900593	13.875469	-0.050512	4.815557
240.203286	7999.936356	13.880474	-0.050469	4.815568
240.507012	7999.935981	13.885479	-0.050526	4.815567
240.242728	7999.929564	13.890483	-0.050477	4.815566
240.227665	7999.961373	13.895488	-0.050474	4.815575
240.358646	7999.899458	13.900493	-0.050499	4.815557
240.278510	7999.915258	13.905498	-0.050484	4.815562
240.567413	7999.913574	13.910503	-0.050538	4.815560
240.389964	7999.918181	13.915507	-0.050505	4.815562
240.377210	7999.926536	13.920512	-0.050503	4.815564
240.301266	7999.919981	13.925517	-0.050489	4.815563
240.257585	7999.924630	13.930522	-0.050481	4.815564
240.233750	7999.925330	13.935527	-0.050477	4.815565
240.362160	7999.924237	13.940531	-0.050501	4.815564
240.375888	7999.949040	13.945536	-0.050504	4.815571
240.303588	7999.934002	13.950541	-0.050491	4.815567
240.365365	7999.951045	13.955546	-0.050503	4.815572
240.235216	7999.937201	13.960551	-0.050479	4.815568
239.881914	7999.884490	13.965555	-0.050413	4.815554
240.165664	7999.940381	13.970560	-0.050466	4.815569
240.410451	7999.915555	13.975565	-0.050512	4.815561
240.142069	7999.904801	13.980570	-0.050462	4.815559
240.372010	7999.922445	13.985575	-0.050505	4.815563
240.412107	7999.913507	13.990579	-0.050513	4.815560
240.261539	7999.932433	13.995584	-0.050485	4.815567
240.118572	7999.920517	14.000589	-0.050459	4.815564
240.252566	7999.948345	14.005594	-0.050484	4.815571
240.318773	7999.941968	14.010599	-0.050497	4.815569
240.076404	7999.909214	14.015603	-0.050452	4.815561
240.160852	7999.953320	14.020608	-0.050468	4.815573
240.402750	7999.938057	14.025613	-0.050513	4.815567
240.371112	7999.922613	14.030618	-0.050507	4.815563
240.193742	7999.934696	14.035623	-0.050474	4.815567
240.135663	7999.876110	14.040627	-0.050464	4.815551
240.211672	7999.936096	14.045632	-0.050478	4.815568
240.297725	7999.903347	14.050637	-0.050494	4.815558
240.241897	7999.928086	14.055642	-0.050484	4.815565
240.306091	7999.935558	14.060647	-0.050497	4.815567
240.147215	7999.918044	14.065651	-0.050467	4.815563
240.289693	7999.947078	14.070656	-0.050494	4.815571
240.411561	7999.906370	14.075661	-0.050517	4.815558
240.272029	7999.900916	14.080666	-0.050491	4.815557
240.377667	7999.916537	14.085671	-0.050511	4.815561
240.460688	7999.904027	14.090675	-0.050527	4.815557
240.431988	7999.917461	14.095680	-0.050522	4.815561
240.297191	7999.929169	14.100685	-0.050497	4.815565
240.342048	7999.937394	14.105690	-0.050505	4.815567
240.409150	7999.959862	14.110695	-0.050518	4.815574
240.279600	7999.924673	14.115699	-0.050494	4.815564
240.012235	7999.944901	14.120704	-0.050445	4.815571
240.194041	7999.912643	14.125709	-0.050479	4.815561
240.140795	7999.925678	14.130714	-0.050469	4.815565
240.094405	7999.933486	14.135719	-0.050461	4.815567
240.213975	7999.935452	14.140723	-0.050483	4.815567
240.227692	7999.970933	14.145728	-0.050486	4.815578
240.284318	7999.917417	14.150733	-0.050497	4.815562
240.181470	7999.925374	14.155738	-0.050478	4.815565
240.410288	7999.949406	14.160743	-0.050521	4.815571
240.265136	7999.895810	14.165747	-0.050494	4.815556
240.439574	7999.925364	14.170752	-0.050526	4.815563
240.613753	7999.908999	14.175757	-0.050559	4.815558
240.525874	7999.921471	14.180762	-0.050543	4.815562
240.397230	7999.941821	14.185767	-0.050519	4.815568
240.278525	7999.899333	14.190771	-0.050497	4.815557
240.432978	7999.942443	14.195776	-0.050526	4.815568
240.279450	7999.923948	14.200781	-0.050498	4.815564
240.248897	7999.912793	14.205786	-0.050493	4.815561
240.345370	7999.942146	14.210791	-0.050511	4.815569
240.273310	7999.896147	14.215795	-0.050498	4.815556
240.283438	7999.939043	14.220800	-0.050500	4.815568
240.330476	7999.930219	14.225805	-0.050509	4.815565
240.314769	7999.704681	14.230810	-0.050506	4.815499

240.261669	7996.427150	14.235815	-0.050494	4.814541
240.247117	7990.781551	14.240819	-0.050488	4.812890
240.343066	7984.044054	14.245824	-0.050502	4.810918
240.326206	7976.662408	14.250829	-0.050494	4.808757
240.308011	7969.041070	14.255834	-0.050486	4.806526
240.392755	7961.216071	14.260839	-0.050497	4.804232
240.310072	7953.374147	14.265843	-0.050476	4.801934
240.300189	7945.354054	14.270848	-0.050470	4.799582
240.188994	7937.447036	14.275853	-0.050444	4.797262
240.047496	7929.417994	14.280858	-0.050413	4.794906
239.920108	7921.399540	14.285863	-0.050384	4.792551
239.845116	7913.306165	14.290867	-0.050365	4.790173
240.033935	7905.416936	14.295872	-0.050395	4.787853
239.835158	7897.390299	14.300877	-0.050353	4.785493
239.864025	7889.399438	14.305882	-0.050354	4.783141
240.002056	7881.402308	14.310887	-0.050374	4.780786
239.909733	7873.402851	14.315891	-0.050352	4.778429
239.933891	7865.402546	14.320896	-0.050352	4.776071
239.943833	7857.421886	14.325901	-0.050349	4.773718
240.064340	7849.341825	14.330906	-0.050366	4.771334
239.964138	7841.407887	14.335911	-0.050342	4.768992
239.763571	7833.383656	14.340915	-0.050300	4.766623
239.889183	7825.342076	14.345920	-0.050318	4.764247
239.709229	7817.439162	14.350925	-0.050280	4.761911
239.319415	7809.307694	14.355930	-0.050202	4.759508
239.657710	7801.451483	14.360935	-0.050260	4.757182
239.346208	7793.333371	14.365939	-0.050197	4.754779
239.386264	7785.304522	14.370944	-0.050200	4.752401
239.301286	7777.324664	14.375949	-0.050179	4.750036
239.390404	7769.305418	14.380954	-0.050191	4.747658
239.399050	7761.335613	14.385959	-0.050187	4.745294
239.278934	7753.357942	14.390963	-0.050160	4.742927
239.376054	7745.335001	14.395968	-0.050173	4.740544
239.009388	7737.371346	14.400973	-0.050100	4.738179
238.844233	7729.289873	14.405978	-0.050064	4.735777
239.132652	7721.364872	14.410983	-0.050113	4.733419
239.141206	7713.294248	14.415987	-0.050109	4.731018
238.978875	7705.341493	14.420992	-0.050074	4.728651
239.000546	7697.303269	14.425997	-0.050073	4.726257
239.006698	7689.275266	14.431002	-0.050069	4.723864
238.980559	7681.341088	14.436007	-0.050060	4.721499
238.777806	7673.282822	14.441011	-0.050017	4.719095
238.812390	7665.387555	14.446016	-0.050018	4.716739
238.790273	7657.352575	14.451021	-0.050009	4.714340
238.689753	7649.322136	14.456026	-0.049985	4.711941
238.770890	7641.262755	14.461031	-0.049996	4.709531
238.547161	7633.291843	14.466035	-0.049949	4.707148
238.699046	7625.273525	14.471040	-0.049972	4.704749
238.589713	7617.313717	14.476045	-0.049947	4.702366
238.454651	7609.279663	14.481050	-0.049917	4.699960
238.587378	7601.368207	14.486055	-0.049937	4.697589
238.558335	7593.260834	14.491059	-0.049926	4.695158
238.641112	7585.309242	14.496064	-0.049937	4.692772
238.379103	7577.279510	14.501069	-0.049883	4.690363
238.231313	7569.244289	14.506074	-0.049850	4.687950
238.404308	7561.295075	14.511079	-0.049877	4.685561
238.451703	7553.339825	14.516083	-0.049881	4.683170
238.249981	7545.324010	14.521088	-0.049839	4.680759
238.168586	7537.308872	14.526093	-0.049819	4.678348
238.219444	7529.262268	14.531098	-0.049823	4.675925
238.081607	7521.242771	14.536103	-0.049792	4.673509
237.930593	7513.140429	14.541107	-0.049759	4.671068
238.000169	7505.165478	14.546112	-0.049767	4.668663
238.016436	7497.256471	14.551117	-0.049765	4.666277
237.963773	7489.228194	14.556122	-0.049751	4.663853
237.799128	7481.285345	14.561127	-0.049715	4.661455
237.873391	7473.228712	14.566131	-0.049724	4.659020
237.969323	7465.231058	14.571136	-0.049737	4.656602
237.728529	7457.240599	14.576141	-0.049687	4.654186
237.819582	7449.199678	14.581146	-0.049699	4.651752
237.870130	7441.189626	14.586151	-0.049703	4.649326
237.850286	7433.260831	14.591155	-0.049695	4.646924
237.926719	7425.175745	14.596160	-0.049704	4.644474
237.772612	7417.238487	14.601165	-0.049670	4.642067
237.744879	7409.228516	14.606170	-0.049660	4.639636
237.748641	7401.284503	14.611175	-0.049656	4.637224
237.788228	7393.217270	14.616179	-0.049658	4.634774
237.622682	7385.172496	14.621184	-0.049622	4.632329
237.478491	7377.209051	14.626189	-0.049590	4.629908
237.651780	7369.206041	14.631194	-0.049618	4.627473
237.555189	7361.205940	14.636199	-0.049595	4.625038
237.234287	7353.198684	14.641203	-0.049530	4.622599
237.292305	7345.194924	14.646208	-0.049536	4.620160
237.415767	7337.243507	14.651213	-0.049554	4.617736
237.311077	7329.184687	14.656218	-0.049529	4.615278
237.254096	7321.170086	14.661223	-0.049514	4.612831
237.187689	7313.123996	14.666227	-0.049496	4.610374
237.265655	7305.177156	14.671232	-0.049506	4.607946
237.133643	7297.162144	14.676237	-0.049476	4.605496
237.086838	7289.159541	14.681242	-0.049463	4.603049
237.328618	7281.191495	14.686247	-0.049503	4.600610
237.033349	7273.210964	14.691251	-0.049443	4.598167
236.928577	7265.197831	14.696256	-0.049418	4.595712
237.091342	7257.132568	14.701261	-0.049444	4.593240
236.895869	7249.075324	14.706266	-0.049402	4.590769
236.620979	7241.140663	14.711271	-0.049346	4.588334
236.692192	7233.117022	14.716275	-0.049354	4.585871
236.762242	7225.141367	14.721280	-0.049362	4.583421
236.617480	7217.161392	14.726285	-0.049331	4.580968
236.464400	7209.132997	14.731290	-0.049297	4.578499
236.897732	7201.197495	14.736295	-0.049373	4.576058
236.761852	7193.112787	14.741299	-0.049342	4.573569
236.691919	7185.101223	14.746304	-0.049324	4.571102
236.692612	7177.068442	14.751309	-0.049320	4.568626
236.402573	7169.113009	14.756314	-0.049261	4.566173
236.631538	7161.138635	14.761319	-0.049298	4.563713
236.314698	7153.160671	14.766323	-0.049234	4.561250
236.581773	7145.113827	14.771328	-0.049279	4.558766
236.307150	7137.162656	14.776333	-0.049223	4.556308
236.052119	7129.100710	14.781338	-0.049170	4.553815
236.326968	7121.130437	14.786343	-0.049217	4.551350
236.249934	7113.096628	14.791347	-0.049197	4.548863
236.244397	7105.122298	14.796352	-0.049191	4.546394
236.248847	7097.124050	14.801357	-0.049187	4.543916
236.154676	7089.113625	14.806362	-0.049165	4.541432
236.125500	7081.156544	14.811367	-0.049154	4.538964
236.262848	7073.152502	14.816371	-0.049175	4.536480
236.265800	7065.125509	14.821376	-0.049170	4.533987
236.255187	7057.081929	14.826381	-0.049163	4.531488
236.117865	7049.064737	14.831386	-0.049133	4.528996
236.222968	7041.141653	14.836391	-0.049147	4.526531
236.097134	7033.083088	14.841395	-0.049119	4.524023
235.900452	7025.146840	14.846400	-0.049077	4.521552
235.820289	7017.123980	14.851405	-0.049058	4.519052
235.747925	7009.140582	14.856410	-0.049039	4.516563
235.713447	7001.141308	14.861415	-0.049028	4.514068
235.512108	6992.978812	14.866419	-0.048985	4.511520
235.610461	6985.015438	14.871424	-0.048998	4.509034
235.563335	6977.074643	14.876429	-0.048985	4.506553
235.510661	6969.019481	14.881434	-0.048970	4.504034
235.557620	6961.091706	14.886439	-0.048974	4.501555
235.394863	6953.103367	14.891443	-0.048938	4.499054
235.277737	6945.117125	14.896448	-0.048912	4.496553
235.543813	6937.056048	14.901453	-0.048956	4.494029
235.537453	6929.009996	14.906458	-0.048950	4.491506
235.212273	6921.027335	14.911463	-0.048884	4.489002
235.203515	6913.030179	14.916467	-0.048878	4.486492
235.342049	6905.068804	14.921472	-0.048899	4.483992
235.114447	6897.111661	14.926477	-0.048851	4.481492
235.086351	6889.040777	14.931482	-0.048841	4.478954
235.268034	6881.131977	14.936487	-0.048870	4.476467
235.002261	6873.054909	14.941491	-0.048816	4.473925
234.962702	6865.040475	14.946496	-0.048803	4.471401
234.872670	6857.030173	14.951501	-0.048781	4.468877
234.860877	6848.986903	14.956506	-0.048774	4.466341
235.050392	6841.040832	14.961511	-0.048805	4.463835
234.717883	6833.101448	14.966515	-0.048738	4.461328
234.822674	6825.005186	14.971520	-0.048752	4.458772
234.712730	6817.070283	14.976525	-0.048727	4.456264
234.622701	6809.014268	14.981530	-0.048705	4.453717
234.770105	6801.011186	14.986535	-0.048727	4.451186
234.764607	6792.995848	14.991539	-0.048721	4.448649
234.595578	6785.025675	14.996544	-0.048685	4.446124
234.792752	6777.039465	15.001549	-0.048717	4.443595
234.753207	6769.028446	15.006554	-0.048704	4.441054
234.730198	6761.038533	15.011559	-0.048695	4.438520
234.382768	6753.028213	15.016563	-0.048625	4.435976
234.274531	6744.994693	15.021568	-0.048600	4.433424
234.405115	6736.954580	15.026573	-0.048620	4.430869
234.129343	6728.957337	15.031578	-0.048563	4.428325
234.167518	6721.009249	15.036583	-0.048565	4.425797
234.191387	6712.971785	15.041587	-0.048565	4.423238
234.285896	6705.006498	15.046592	-0.048577	4.420702
234.100635	6697.025538	15.051597	-0.048538	4.418157
233.991923	6689.007945	15.056602	-0.048513	4.415600
234.234582	6681.013027	15.061607	-0.048553	4.413050
234.117879	6672.965765	15.066611	-0.048526	4.410480
234.175991	6665.002516	15.071616	-0.048532	4.407937
234.057953	6656.977376	15.076621	-0.048505	4.405371
233.852950	6649.030611	15.081626	-0.048462	4.402829
234.145138	6641.016868	15.086631	-0.048511	4.400266
234.017995	6633.025456	15.091635	-0.048483	4.397706
233.715437	6625.024201	15.096640	-0.048421	4.395141
233.820318	6616.962321	15.101645	-0.048436	4.392558
233.710450	6608.915696	15.106650	-0.048411	4.389976
233.848491	6600.983277	15.111655	-0.048431	4.387431
233.801437	6592.969287	15.116659	-0.048418	4.384857
233.759356	6585.001708	15.121664	-0.048405	4.382297
233.644368	6577.003244	15.126669	-0.048378	4.379725
233.650324	6569.046120	15.131674	-0.048374	4.377165
233.588241	6561.022195	15.136679	-0.048358	4.374582
233.664556	6552.948120	15.141683	-0.048367	4.371982
233.562590	6544.956774	15.146688	-0.048343	4.369406
233.596308	6537.016955	15.151693	-0.048344	4.366846
233.406524	6528.966157	15.156698	-0.048304	4.364247
233.432236	6521.023340	15.161703	-0.048304	4.361683
233.367398	6512.993257	15.166707	-0.048287	4.359088
233.393104	6505.052124	15.171712	-0.048287	4.356522
233.375743	6496.997835	15.176717	-0.048279	4.353917
233.204626	6488.853128	15.181722	-0.048242	4.351280
233.171830	6480.927469	15.186727	-0.048231	4.348713
233.120253	6472.918275	15.191731	-0.048216	4.346118
233.001971	6464.970160	15.196736	-0.048189	4.343541
232.925567	6456.958586	15.201741	-0.048170	4.340941
232.803292	6448.983594	15.206746	-0.048142	4.338352
232.912074	6440.982515	15.211751	-0.048157	4.335754
232.838534	6432.945965	15.216755	-0.048139	4.333142
232.909009	6424.923629	15.221760	-0.048147	4.330534
232.882552	6416.983063	15.226765	-0.048137	4.327950
232.634936	6408.958223	15.231770	-0.048086	4.325336
232.559665	6401.012082	15.236775	-0.048067	4.322747
232.750446	6392.936417	15.241779	-0.048097	4.320116
232.588662	6384.984646	15.246784	-0.048062	4.317521
232.582832	6376.981542	15.251789	-0.048056	4.314909
232.547228	6368.907523	15.256794	-0.048044	4.312272
232.647525	6360.912654	15.261799	-0.048058	4.309661
232.496669	6352.960024	15.266803	-0.048025	4.307059
232.347721	6344.911095	15.271808	-0.047992	4.304425
232.282323	6336.966221	15.276813	-0.047975	4.301824
232.252488	6328.912891	15.281818	-0.047965	4.299186
232.366539	6320.970529	15.286823	-0.047981	4.296583
232.213168	6312.965274	15.291827	-0.047947	4.293957
232.232797	6304.941684	15.296832	-0.047946	4.291324
232.184128	6296.939928	15.301837	-0.047932	4.288696
232.010019	6288.916809	15.306842	-0.047895	4.286059
232.244246	6280.928236	15.311847	-0.047933	4.283435
232.028349	6272.950267	15.316851	-0.047888	4.280808
232.042967	6264.913522	15.321856	-0.047886	4.278163
232.112355	6256.932448	15.326861	-0.047894	4.275535
232.124604	6248.883885	15.331866	-0.047891	4.272883
231.812341	6240.900908	15.336871	-0.047828	4.270247
231.842463	6232.880819	15.341875	-0.047829	4.267601
231.796447	6224.869623	15.346880	-0.047815	4.264955
231.743512	6216.926900	15.351885	-0.047800	4.262331
231.520716	6208.869080	15.356890	-0.047754	4.259665
231.594225	6200.982865	15.361895	-0.047762	4.257057
231.431300	6192.892975	15.366899	-0.047727	4.254377
231.367758	6184.874293	15.371904	-0.047710	4.251721
231.508017	6176.876639	15.376909	-0.047731	4.249072
231.578836	6168.935751	15.381914	-0.047740	4.246439
231.509307	6160.920961	15.386919	-0.047722	4.243779
231.400845	6152.914220	15.391923	-0.047697	4.241119
231.476395	6144.916679	15.396928	-0.047706	4.238462
231.412180	6136.947870	15.401933	-0.047689	4.235812
231.339830	6128.908325	15.406938	-0.047670	4.233137
231.345429	6120.933503	15.411943	-0.047666	4.230483
231.323378	6112.894231	15.416947	-0.047657	4.227805
231.378030	6104.916792	15.421952	-0.047662	4.225146
231.430056	6096.970639	15.426957	-0.047667	4.222496
231.212142	6088.917845	15.431962	-0.047622	4.219807
231.226856	6080.995977	15.436967	-0.047619	4.217162
231.258936	6072.940319	15.441971	-0.047620	4.214470
231.176663	6064.928765	15.446976	-0.047600	4.211791
231.143133	6056.928315	15.451981	-0.047589	4.209113
230.765672	6048.957599	15.456986	-0.047514	4.206441
230.939645	6040.931155	15.461991	-0.047541	4.203754
230.887497	6032.950381	15.466995	-0.047526	4.201078
230.804407	6024.962669	15.472000	-0.047506	4.198398
230.803169	6017.002608	15.477005	-0.047501	4.195726
230.850274	6008.876033	15.482010	-0.047504	4.192997
230.738202	6000.830422	15.487015	-0.047478	4.190292
230.626212	5992.895852	15.492019	-0.047453	4.187622
230.671944	5984.862035	15.497024	-0.047456	4.184919
230.709738	5976.932828	15.502029	-0.047458	4.182250
230.548679	5968.923515	15.507034	-0.047423	4.179549
230.683345	5960.944846	15.512039	-0.047443	4.176860
230.380708	5952.913659	15.517043	-0.047382	4.174147
230.317887	5944.883499	15.522048	-0.047365	4.171436
230.468646	5936.880046	15.527053	-0.047388	4.168733
230.361032	5928.893241	15.532058	-0.047363	4.166032
230.420002	5920.924450	15.537063	-0.047369	4.163337
230.294655	5912.891504	15.542067	-0.047341	4.160617
230.226833	5904.935604	15.547072	-0.047324	4.157921
230.221061	5896.953284	15.552077	-0.047318	4.155216
229.909703	5888.861661	15.557082	-0.047254	4.152468
230.035309	5880.896334	15.562087	-0.047273	4.149766
230.324576	5872.886278	15.567091	-0.047322	4.147049
230.102646	5864.872818	15.572096	-0.047275	4.144323
230.065874	5856.937987	15.577101	-0.047264	4.141625
230.111726	5848.907254	15.582106	-0.047267	4.138893
230.085682	5840.938477	15.587111	-0.047257	4.136179
229.739735	5832.871102	15.592115	-0.047188	4.133426
229.967749	5824.876259	15.597120	-0.047225	4.130703
229.994824	5816.933281	15.602125	-0.047226	4.127993
229.710908	5808.920095	15.607130	-0.047168	4.125254
229.841309	5800.947296	15.612135	-0.047187	4.122532
229.700325	5792.898499	15.617139	-0.047156	4.119779
229.701306	5784.955680	15.622144	-0.047151	4.117062
229.730386	5776.941383	15.627149	-0.047151	4.114319
229.594346	5768.834785	15.632154	-0.047121	4.111540
229.698665	5760.881226	15.637159	-0.047136	4.108815
229.537283	5752.859319	15.642163	-0.047100	4.106062
229.330061	5744.902817	15.647168	-0.047057	4.103328
229.532013	5736.884166	15.652173	-0.047090	4.100577
229.312149	5728.931633	15.657178	-0.047044	4.097841
229.428167	5720.921541	15.662183	-0.047060	4.095087
229.322979	5712.929971	15.667187	-0.047036	4.092336
229.289162	5704.906589	15.672192	-0.047024	4.089572
229.193416	5696.964449	15.677197	-0.047002	4.086834
229.145278	5688.893659	15.682202	-0.046988	4.084050
229.253165	5680.975930	15.687207	-0.047003	4.081319
228.880060	5672.950766	15.692211	-0.046928	4.078543
228.855080	5664.962382	15.697216	-0.046919	4.075782
228.908247	5656.937460	15.702221	-0.046924	4.073008
228.825099	5648.876626	15.707226	-0.046903	4.070217
228.918660	5640.950248	15.712231	-0.046916	4.067474
228.924977	5632.927380	15.717235	-0.046912	4.064694
228.714718	5624.970232	15.722240	-0.046868	4.061932
228.838247	5616.947209	15.727245	-0.046886	4.059150
228.837893	5608.981534	15.732250	-0.046881	4.056384
228.939355	5600.946084	15.737255	-0.046895	4.053594
228.635194	5592.893661	15.742259	-0.046833	4.050789
228.818649	5584.912499	15.747264	-0.046862	4.048015
228.854973	5576.939385	15.752269	-0.046864	4.045240
228.806607	5568.948466	15.757274	-0.046850	4.042455
228.518878	5560.954513	15.762279	-0.046791	4.039664
228.552532	5552.988194	15.767283	-0.046793	4.036885
228.647823	5544.919215	15.772288	-0.046805	4.034069
228.444168	5536.849137	15.777293	-0.046762	4.031246
228.401918	5528.862579	15.782298	-0.046750	4.028453
228.335225	5520.928146	15.787303	-0.046732	4.025676
228.181493	5512.936188	15.792307	-0.046699	4.022876
228.215851	5504.880999	15.797312	-0.046700	4.020054
228.392077	5496.944455	15.802317	-0.046728	4.017274
228.077261	5488.897304	15.807322	-0.046664	4.014446
228.074751	5480.911343	15.812327	-0.046659	4.011642
228.068460	5472.883176	15.817331	-0.046653	4.008822
228.002679	5464.920159	15.822336	-0.046635	4.006021
227.955825	5456.953906	15.827341	-0.046622	4.003217
228.026390	5448.913464	15.832346	-0.046630	4.000388
228.033524	5440.963961	15.837351	-0.046626	3.997587
227.812385	5432.979158	15.842355	-0.046580	3.994768
227.900170	5424.899186	15.847360	-0.046591	3.991918
227.954055	5416.893696	15.852365	-0.046596	3.989093
227.661576	5408.886976	15.857370	-0.046537	3.986259
227.772310	5400.934364	15.862375	-0.046553	3.983449
227.584009	5392.938698	15.867379	-0.046513	3.980617
227.834467	5384.908796	15.872384	-0.046554	3.977777
227.740941	5376.938635	15.877389	-0.046532	3.974952
227.648857	5368.930993	15.882394	-0.046510	3.972111
227.832868	5360.940614	15.887399	-0.046539	3.969278
227.687268	5352.968099	15.892403	-0.046507	3.966445
227.458441	5344.957039	15.897408	-0.046459	3.963594
227.505864	5336.993828	15.902413	-0.046463	3.960763
227.361621	5328.992948	15.907418	-0.046431	3.957913
227.489189	5321.013621	15.912423	-0.046450	3.955074
227.370435	5312.960910	15.917427	-0.046423	3.952202
227.190011	5304.930253	15.922432	-0.046385	3.949335
227.258726	5296.969345	15.927437	-0.046392	3.946495
227.034384	5288.963940	15.932442	-0.046346	3.943631
227.082736	5280.967537	15.937447	-0.046350	3.940774
227.003342	5272.986760	15.942451	-0.046330	3.937918
226.918682	5264.991150	15.947456	-0.046309	3.935055
227.181503	5257.006647	15.952461	-0.046353	3.932199
226.988251	5248.981126	15.957466	-0.046312	3.929319
226.842676	5241.016590	15.962471	-0.046280	3.926459
226.742052	5232.986099	15.967475	-0.046256	3.923574
226.819259	5224.971629	15.972480	-0.046266	3.920697
226.719341	5217.076227	15.977485	-0.046242	3.917856
226.569417	5209.021752	15.982490	-0.046209	3.914955
226.729483	5201.001572	15.987495	-0.046234	3.912071
226.648917	5192.981484	15.992499	-0.046214	3.909179
226.532802	5184.983062	15.997504	-0.046187	3.906293
226.611585	5177.004682	16.002509	-0.046197	3.903416
226.465756	5168.992900	16.007514	-0.046165	3.900520
226.485743	5161.024213	16.012519	-0.046164	3.897640
226.387807	5152.989092	16.017523	-0.046141	3.894732
226.368209	5144.990373	16.022528	-0.046132	3.891837
226.341998	5136.972124	16.027533	-0.046122	3.888932
226.275186	5128.981845	16.032538	-0.046105	3.886035
226.311107	5121.026489	16.037543	-0.046106	3.883150
226.418919	5113.010427	16.042547	-0.046121	3.880242
226.293828	5105.001689	16.047552	-0.046093	3.877330
226.445814	5097.029571	16.052557	-0.046117	3.874435
226.338106	5088.762623	16.057562	-0.046091	3.871425
226.242090	5080.875212	16.062567	-0.046069	3.868551
225.946737	5072.911228	16.067571	-0.046009	3.865643
226.086958	5064.954343	16.072576	-0.046030	3.862744
226.034826	5056.991710	16.077581	-0.046015	3.859837
225.988554	5049.001455	16.082586	-0.046001	3.856918
226.000107	5041.002122	16.087591	-0.045999	3.853995
226.134398	5032.973037	16.092595	-0.046019	3.851061
225.859731	5024.989852	16.097600	-0.045963	3.848133
225.812138	5017.032546	16.102605	-0.045949	3.845217
225.752080	5009.051357	16.107610	-0.045933	3.842290
225.576907	5001.032575	16.112615	-0.045895	3.839344
225.593079	4993.090817	16.117619	-0.045893	3.836429
225.660536	4985.040081	16.122624	-0.045901	3.833472
225.716011	4977.029312	16.127629	-0.045906	3.830527
225.438307	4969.045392	16.132634	-0.045849	3.827583
225.772375	4961.004752	16.137639	-0.045906	3.824629
225.668172	4953.098661	16.142643	-0.045882	3.821713
225.357228	4945.098048	16.147648	-0.045819	3.818755
225.660986	4937.102040	16.152653	-0.045871	3.815809
225.635528	4929.048400	16.157658	-0.045861	3.812834
225.520674	4921.094052	16.162663	-0.045835	3.809890
225.254535	4913.099079	16.167667	-0.045780	3.806926
225.451159	4905.075748	16.172672	-0.045812	3.803959
225.356092	4897.156589	16.177677	-0.045789	3.801022
225.050433	4889.128123	16.182682	-0.045727	3.798038
225.103314	4881.110108	16.187687	-0.045732	3.795063
225.078756	4873.083639	16.192691	-0.045723	3.792081
225.003097	4865.038844	16.197696	-0.045703	3.789089
224.905203	4857.111652	16.202701	-0.045680	3.786137
224.667086	4849.067513	16.207706	-0.045631	3.783136
224.839607	4841.119056	16.212711	-0.045658	3.780178
224.829333	4833.105778	16.217715	-0.045651	3.777190
224.674231	4825.108456	16.222720	-0.045617	3.774201
224.808812	4817.109139	16.227725	-0.045637	3.771216
224.795324	4809.093401	16.232730	-0.045630	3.768219
224.884537	4801.061925	16.237735	-0.045642	3.765217
224.829410	4793.124021	16.242739	-0.045626	3.762243
224.515846	4785.123370	16.247744	-0.045563	3.759238
224.324446	4777.182468	16.252749	-0.045522	3.756256
224.445064	4769.123053	16.257754	-0.045540	3.753234
224.611382	4761.097984	16.262759	-0.045566	3.750223
224.367887	4753.108138	16.267763	-0.045515	3.747214
224.440350	4745.086833	16.272768	-0.045524	3.744198
224.470232	4737.164975	16.277773	-0.045525	3.741215
224.258498	4729.135424	16.282778	-0.045480	3.738185
224.107390	4721.164928	16.287783	-0.045447	3.735175
224.237186	4713.147610	16.292787	-0.045466	3.732152
224.173244	4705.123418	16.297792	-0.045449	3.729119
224.302989	4697.180959	16.302797	-0.045469	3.726120
223.837401	4689.193768	16.307802	-0.045377	3.723086
224.122865	4681.199825	16.312807	-0.045425	3.720066
224.071856	4673.215745	16.317811	-0.045411	3.717039
224.040457	4665.167822	16.322816	-0.045400	3.713986
223.954304	4657.111989	16.327821	-0.045379	3.710925
223.674907	4649.132865	16.332826	-0.045322	3.707887
223.757063	4641.118855	16.337831	-0.045332	3.704842
223.765543	4633.181811	16.342835	-0.045329	3.701822
223.784047	4625.194873	16.347840	-0.045327	3.698780
223.776062	4617.246531	16.352845	-0.045321	3.695750
223.496855	4609.212936	16.357850	-0.045264	3.692679
223.616879	4601.195787	16.362855	-0.045281	3.689621
223.397005	4593.238754	16.367859	-0.045235	3.686574
223.523077	4585.245050	16.372864	-0.045254	3.683520
223.683721	4577.276823	16.377869	-0.045279	3.680475
223.550713	4569.262219	16.382874	-0.045249	3.677401
223.441777	4561.248699	16.387879	-0.045224	3.674326
223.294512	4553.235569	16.392883	-0.045191	3.671247
223.402132	4545.221826	16.397888	-0.045206	3.668172
223.257441	4537.266703	16.402893	-0.045174	3.665111
223.154396	4529.261938	16.407898	-0.045150	3.662029
223.308726	4521.256216	16.412903	-0.045174	3.658951
223.272373	4513.261242	16.417907	-0.045162	3.655869
223.087652	4505.245939	16.422912	-0.045123	3.652773
223.108423	4497.277617	16.427917	-0.045122	3.649698
223.070428	4489.257843	16.432922	-0.045110	3.646598
223.154677	4481.259898	16.437927	-0.045120	3.643508
223.114629	4473.295030	16.442931	-0.045108	3.640425
222.928790	4465.314798	16.447936	-0.045068	3.637329
222.817211	4457.315361	16.452941	-0.045043	3.634225
222.730854	4449.288079	16.457946	-0.045021	3.631109
222.978408	4441.264511	16.462951	-0.045063	3.628000
222.784261	4433.262581	16.467955	-0.045021	3.624885
222.621894	4425.312724	16.472960	-0.044986	3.621788
222.763032	4417.303489	16.477965	-0.045008	3.618674
222.700805	4409.328261	16.482970	-0.044991	3.615564
222.682956	4401.331179	16.487975	-0.044983	3.612445
222.751744	4393.311682	16.492979	-0.044991	3.609317
222.519749	4385.337295	16.497984	-0.044942	3.606195
222.569794	4377.380920	16.502989	-0.044947	3.603086
222.248869	4369.372619	16.507994	-0.044882	3.599943
222.392350	4361.420200	16.512999	-0.044904	3.596832
222.391296	4353.392661	16.518003	-0.044899	3.593685
222.248311	4345.346608	16.523008	-0.044867	3.590524
222.055187	4337.404310	16.528013	-0.044826	3.587400
222.104792	4329.364085	16.533018	-0.044830	3.584241
222.062952	4321.439908	16.538023	-0.044818	3.581122
221.984392	4313.423097	16.543027	-0.044798	3.577963
221.912580	4305.416872	16.548032	-0.044780	3.574806
221.964611	4297.439535	16.553037	-0.044784	3.571661
221.937616	4289.383323	16.558042	-0.044774	3.568480
221.922049	4281.422710	16.563047	-0.044766	3.565334
221.836074	4273.443565	16.568051	-0.044745	3.562175
221.687645	4265.433596	16.573056	-0.044713	3.559000
221.941316	4257.458482	16.578061	-0.044755	3.555848
221.629784	4249.378965	16.583066	-0.044692	3.552635
221.557484	4241.370025	16.588071	-0.044674	3.549454
221.425448	4233.414404	16.593075	-0.044644	3.546289
221.410539	4225.400655	16.598080	-0.044636	3.543102
221.475304	4217.445371	16.603085	-0.044643	3.539938
221.252807	4209.474191	16.608090	-0.044597	3.536756
221.469720	4201.455146	16.613095	-0.044632	3.533566
221.353055	4193.456811	16.618099	-0.044606	3.530370
221.221686	4185.467674	16.623104	-0.044576	3.527175
221.366952	4177.469444	16.628109	-0.044598	3.523982
221.282153	4169.506117	16.633114	-0.044578	3.520793
221.439239	4161.498799	16.638119	-0.044602	3.517591
221.036247	4153.539373	16.643123	-0.044522	3.514388
221.253877	4145.487515	16.648128	-0.044557	3.511163
221.304838	4137.479129	16.653133	-0.044562	3.507949
221.180283	4129.452053	16.658138	-0.044534	3.504718
221.130028	4121.536808	16.663143	-0.044519	3.501532
221.253908	4113.563342	16.668147	-0.044537	3.498325
220.910704	4105.587866	16.673152	-0.044469	3.495099
221.005548	4097.594196	16.678157	-0.044481	3.491877
221.117060	4089.554017	16.683162	-0.044497	3.488633
220.847909	4081.566597	16.688167	-0.044442	3.485396
220.963880	4073.621970	16.693171	-0.044459	3.482185
220.956240	4065.627337	16.698176	-0.044452	3.478947
220.987926	4057.639354	16.703181	-0.044453	3.475711
220.742688	4049.586159	16.708186	-0.044402	3.472435
220.782153	4041.568764	16.713191	-0.044405	3.469181
220.819214	4033.602059	16.718195	-0.044407	3.465943
220.703494	4025.625845	16.723200	-0.044380	3.462694
220.661980	4017.638207	16.728205	-0.044368	3.459440
220.522819	4009.675132	16.733210	-0.044337	3.456189
220.667569	4001.629476	16.738215	-0.044359	3.452911
220.712745	3993.604776	16.743219	-0.044362	3.449635
220.551846	3985.647088	16.748224	-0.044327	3.446377
220.515573	3977.689194	16.753229	-0.044315	3.443119
220.267832	3969.677555	16.758234	-0.044264	3.439830
220.224239	3961.722536	16.763239	-0.044251	3.436567
220.410733	3953.666591	16.768243	-0.044281	3.433267
220.245691	3945.650104	16.773248	-0.044245	3.429969
220.112158	3937.695746	16.778253	-0.044215	3.426694
220.059613	3929.693877	16.783258	-0.044201	3.423399
220.083581	3921.717676	16.788263	-0.044200	3.420114
219.884789	3913.770554	16.793267	-0.044158	3.416830
220.264764	3905.697832	16.798272	-0.044224	3.413511
220.223360	3897.731193	16.803277	-0.044211	3.410218
219.937959	3889.738232	16.808282	-0.044153	3.406903
219.928914	3881.740709	16.813287	-0.044146	3.403592
220.073646	3873.790093	16.818291	-0.044168	3.400303
219.964820	3865.827710	16.823296	-0.044143	3.396997
219.861363	3857.813306	16.828301	-0.044119	3.393666
219.593198	3849.693782	16.833306	-0.044064	3.390282
219.648162	3841.754031	16.838311	-0.044069	3.386981
219.655487	3833.765324	16.843315	-0.044066	3.383655
219.633241	3825.804196	16.848320	-0.044057	3.380336
219.572398	3817.852683	16.853325	-0.044040	3.377017
219.319137	3809.838720	16.858330	-0.043988	3.373661
219.450125	3801.825464	16.863335	-0.044008	3.370316
219.509723	3793.834411	16.868339	-0.044014	3.366974
219.303604	3785.854662	16.873344	-0.043970	3.363624
219.263015	3777.887356	16.878349	-0.043958	3.360282
219.216352	3769.903989	16.883354	-0.043944	3.356929
219.492713	3761.876252	16.888359	-0.043991	3.353567
219.180680	3753.872429	16.893363	-0.043927	3.350189
219.140189	3745.862199	16.898368	-0.043915	3.346816
219.218359	3737.894194	16.903373	-0.043925	3.343461
219.042156	3729.937795	16.908378	-0.043887	3.340098
218.922846	3721.961627	16.913383	-0.043860	3.336726
218.908271	3713.942349	16.918387	-0.043852	3.333335
218.919546	3705.887677	16.923392	-0.043849	3.329928
218.849247	3697.958181	16.928397	-0.043831	3.326567
218.792408	3689.955331	16.933402	-0.043815	3.323171
218.883390	3681.994710	16.938407	-0.043827	3.319796
218.880107	3674.027707	16.943411	-0.043822	3.316411
218.717320	3665.995657	16.948416	-0.043787	3.312989
218.847082	3657.973140	16.953421	-0.043806	3.309579
218.561223	3649.991412	16.958426	-0.043747	3.306166
218.522631	3642.022354	16.963431	-0.043735	3.302765
218.566896	3634.048278	16.968435	-0.043739	3.299362
218.558197	3626.079126	16.973440	-0.043732	3.295955
218.462229	3618.080843	16.978445	-0.043709	3.292528
218.373272	3610.055342	16.983450	-0.043688	3.289087
218.459731	3602.077053	16.988455	-0.043699	3.285669
218.330200	3594.101819	16.993459	-0.043670	3.282240
218.123862	3586.117246	16.998464	-0.043626	3.278801
218.432809	3578.135767	17.003469	-0.043679	3.275380
218.358956	3570.098728	17.008474	-0.043660	3.271916
218.246605	3562.117898	17.013479	-0.043634	3.268471
218.017960	3554.144585	17.018483	-0.043587	3.265021
217.857590	3546.155511	17.023488	-0.043552	3.261564
217.962522	3538.191077	17.028493	-0.043566	3.258124
217.906107	3530.164778	17.033498	-0.043551	3.254647
217.845674	3522.163297	17.038503	-0.043535	3.251176
218.061236	3514.185929	17.043507	-0.043570	3.247724
218.049274	3506.183370	17.048512	-0.043563	3.244248
218.088889	3498.257823	17.053517	-0.043565	3.240804
217.932734	3490.262071	17.058522	-0.043531	3.237318
217.981888	3482.245891	17.063527	-0.043535	3.233827
217.864809	3474.193747	17.068531	-0.043508	3.230310
217.750311	3466.205215	17.073536	-0.043482	3.226817
217.435703	3458.263393	17.078541	-0.043419	3.223333
217.346211	3450.263568	17.083546	-0.043397	3.219828
217.537018	3442.300290	17.088551	-0.043427	3.216347
217.487742	3434.299848	17.093555	-0.043413	3.212837
217.471782	3426.279448	17.098560	-0.043405	3.209315
217.583917	3418.323194	17.103565	-0.043421	3.205823
217.262921	3410.342845	17.108570	-0.043357	3.202298
217.157637	3402.378588	17.113575	-0.043332	3.198785
217.116989	3394.413447	17.118579	-0.043319	3.195271
217.237464	3386.342073	17.123584	-0.043337	3.191713
217.115549	3378.391754	17.128589	-0.043309	3.188194
217.081038	3370.372091	17.133594	-0.043298	3.184644
217.164199	3362.407868	17.138599	-0.043308	3.181120
217.118846	3354.439451	17.143603	-0.043295	3.177585
216.966428	3346.438926	17.148608	-0.043262	3.174027
216.895050	3338.450865	17.153613	-0.043243	3.170474
216.845647	3330.457049	17.158618	-0.043229	3.166915
216.808798	3322.476633	17.163623	-0.043217	3.163359
216.786520	3314.494702	17.168627	-0.043208	3.159798
216.795618	3306.530611	17.173632	-0.043205	3.156243
216.587565	3298.519858	17.178637	-0.043161	3.152654
216.441128	3290.509528	17.183642	-0.043129	3.149063
216.559642	3282.497115	17.188647	-0.043146	3.145479
216.446530	3274.561706	17.193651	-0.043120	3.141915
216.240336	3266.595856	17.198656	-0.043077	3.138330
216.334548	3258.580496	17.203661	-0.043089	3.134731
216.455704	3250.561933	17.208666	-0.043107	3.131128
216.343895	3242.590794	17.213671	-0.043081	3.127532
216.190756	3234.631589	17.218675	-0.043048	3.123935
216.256547	3226.637805	17.223680	-0.043055	3.120328
216.513082	3218.668094	17.228685	-0.043098	3.116736
216.254939	3210.656667	17.233690	-0.043045	3.113099
216.314060	3202.622395	17.238695	-0.043051	3.109461
216.133864	3194.676439	17.243699	-0.043012	3.105848
216.099326	3186.686766	17.248704	-0.043001	3.102217
216.145270	3178.719659	17.253709	-0.043004	3.098596
215.932458	3170.750851	17.258714	-0.042960	3.094958
215.769538	3162.742003	17.263719	-0.042924	3.091300
215.747087	3154.757257	17.268723	-0.042915	3.087655
215.723502	3146.759533	17.273728	-0.042906	3.084000
215.721255	3138.803246	17.278733	-0.042900	3.080360
215.527872	3130.852603	17.283738	-0.042859	3.076710
215.597106	3122.795649	17.288743	-0.042867	3.073019
215.641118	3114.751591	17.293747	-0.042871	3.069328
215.412916	3106.778917	17.298752	-0.042823	3.065653
215.498570	3098.843486	17.303757	-0.042834	3.062005
215.441314	3090.840014	17.308762	-0.042818	3.058315
215.484675	3082.862283	17.313767	-0.042822	3.054637
215.309367	3074.882177	17.318771	-0.042784	3.050943
215.193175	3066.898313	17.323776	-0.042757	3.047246
215.227657	3058.934927	17.328781	-0.042759	3.043560
215.121174	3050.946614	17.333786	-0.042734	3.039852
215.073710	3042.997619	17.338791	-0.042720	3.036161
215.044086	3034.981262	17.343795	-0.042710	3.032435
215.050971	3026.968295	17.348800	-0.042706	3.028707
215.140034	3018.994807	17.353805	-0.042718	3.024997
214.915695	3011.041029	17.358810	-0.042671	3.021277
214.955186	3003.046185	17.363815	-0.042673	3.017545
214.908379	2995.058910	17.368819	-0.042660	3.013808
215.029561	2987.025274	17.373824	-0.042677	3.010054
215.000201	2979.083334	17.378829	-0.042667	3.006330
214.804452	2971.097645	17.383834	-0.042625	3.002572
214.959446	2963.126863	17.388839	-0.042649	2.998835
214.966203	2955.172994	17.393843	-0.042646	2.995093
214.775933	2947.148599	17.398848	-0.042605	2.991303
214.610403	2939.174181	17.403853	-0.042569	2.987534
214.616170	2931.158669	17.408858	-0.042565	2.983749
214.633923	2923.206813	17.413863	-0.042564	2.979990
214.561216	2915.246959	17.418867	-0.042545	2.976217
214.496877	2907.231186	17.423872	-0.042528	2.972414
214.548941	2899.252019	17.428877	-0.042533	2.968629
214.428989	2891.264697	17.433882	-0.042506	2.964827
214.515060	2883.292420	17.438887	-0.042517	2.961037
214.330279	2875.354230	17.443891	-0.042477	2.957246
214.076905	2867.350017	17.448896	-0.042425	2.953414
214.148525	2859.337533	17.453901	-0.042434	2.949589
214.201191	2851.358325	17.458906	-0.042438	2.945775
214.265154	2843.362796	17.463911	-0.042445	2.941949
214.171311	2835.423403	17.468915	-0.042423	2.938136
213.956799	2827.431485	17.473920	-0.042378	2.934287
214.131115	2819.426590	17.478925	-0.042406	2.930447
213.947492	2811.456935	17.483930	-0.042366	2.926600
213.917950	2803.477115	17.488935	-0.042356	2.922751
213.915919	2795.519025	17.493939	-0.042351	2.918910
213.851699	2787.529190	17.498944	-0.042334	2.915044
213.865427	2779.455046	17.503949	-0.042331	2.911136
213.704063	2771.495349	17.508954	-0.042296	2.907270
213.835009	2763.508920	17.513959	-0.042316	2.903401
213.624653	2755.579792	17.518963	-0.042271	2.899536
213.444935	2747.624617	17.523968	-0.042233	2.895655
213.525923	2739.600057	17.528973	-0.042243	2.891749
213.462526	2731.622163	17.533978	-0.042226	2.887853
213.442100	2723.650286	17.538983	-0.042218	2.883956
213.553223	2715.661130	17.543987	-0.042233	2.880054
213.522532	2707.695403	17.548992	-0.042223	2.876149
213.363000	2699.728857	17.553997	-0.042188	2.872232
213.240064	2691.710738	17.559002	-0.042160	2.868286
213.261123	2683.742718	17.564007	-0.042159	2.864367
213.170450	2675.795628	17.569011	-0.042137	2.860448
213.087646	2667.816220	17.574016	-0.042117	2.856507
213.286865	2659.814769	17.579021	-0.042149	2.852565
213.072022	2651.827574	17.584026	-0.042104	2.848602
212.740167	2643.895723	17.589031	-0.042037	2.844654
212.902675	2635.911423	17.594035	-0.042063	2.840703
212.873703	2627.918457	17.599040	-0.042052	2.836731
212.780509	2619.950910	17.604045	-0.042030	2.832762
212.721583	2611.945580	17.609050	-0.042014	2.828771
212.770452	2603.943642	17.614055	-0.042018	2.824782
212.691541	2595.996953	17.619059	-0.041998	2.820807
212.641648	2588.015773	17.624064	-0.041984	2.816812
212.644902	2580.044823	17.629069	-0.041980	2.812819
212.658453	2572.036123	17.634074	-0.041977	2.808802
212.744702	2564.042915	17.639079	-0.041988	2.804791
212.740550	2556.106867	17.644083	-0.041983	2.800798
212.383458	2548.154822	17.649088	-0.041911	2.796771
212.358306	2540.178470	17.654093	-0.041902	2.792744
212.404184	2532.162794	17.659098	-0.041905	2.788697
212.264588	2524.188906	17.664103	-0.041874	2.784653
212.402112	2516.246755	17.669107	-0.041895	2.780637
212.074700	2508.273068	17.674112	-0.041829	2.776571
212.241617	2500.263967	17.679117	-0.041855	2.772510
212.074294	2492.278009	17.684122	-0.041819	2.768435
212.046618	2484.304067	17.689127	-0.041809	2.764368
211.964440	2476.377599	17.694131	-0.041789	2.760317
211.889030	2468.388793	17.699136	-0.041769	2.756228
211.889484	2460.342026	17.704141	-0.041765	2.752108
211.758432	2452.337412	17.709146	-0.041735	2.747995
211.987318	2444.347904	17.714151	-0.041773	2.743906
211.900604	2436.415392	17.719155	-0.041752	2.739821
211.794073	2428.463189	17.724160	-0.041727	2.735718
211.645378	2420.491693	17.729165	-0.041694	2.731597
211.577235	2412.492543	17.734170	-0.041677	2.727460
211.518956	2404.534537	17.739175	-0.041661	2.723339
211.628003	2396.569858	17.744179	-0.041676	2.719218
211.634032	2388.599439	17.749184	-0.041672	2.715082
211.628904	2380.613088	17.754189	-0.041666	2.710930
211.467545	2372.629528	17.759194	-0.041631	2.706764
211.545094	2364.674548	17.764199	-0.041641	2.702621
211.596320	2356.717560	17.769203	-0.041645	2.698469
211.245910	2348.750165	17.774208	-0.041575	2.694280
211.211125	2340.748959	17.779213	-0.041564	2.690086
211.258742	2332.760401	17.784218	-0.041568	2.685898
211.273413	2324.813193	17.789223	-0.041565	2.681723
211.304273	2316.859198	17.794227	-0.041566	2.677539
211.300077	2308.860913	17.799232	-0.041561	2.673323
211.218377	2300.872849	17.804237	-0.041540	2.669100
210.999872	2292.891709	17.809242	-0.041495	2.664866
211.064044	2284.933669	17.814247	-0.041502	2.660655
211.024650	2276.976725	17.819251	-0.041489	2.656432
210.918992	2268.984784	17.824256	-0.041465	2.652179
210.673339	2261.042803	17.829261	-0.041414	2.647936
210.523199	2253.072414	17.834266	-0.041381	2.643678
210.572911	2245.099151	17.839271	-0.041385	2.639424
210.585610	2237.139181	17.844275	-0.041383	2.635169
210.712249	2229.118315	17.849280	-0.041401	2.630881
210.472512	2221.192610	17.854285	-0.041352	2.626613
210.399562	2213.211985	17.859290	-0.041333	2.622320
210.441689	2205.242674	17.864295	-0.041336	2.618033
210.374794	2197.283711	17.869299	-0.041319	2.613737
210.216187	2189.277346	17.874304	-0.041284	2.609403
210.485300	2181.299192	17.879309	-0.041329	2.605106
210.209871	2173.368806	17.884314	-0.041273	2.600790
210.212522	2165.405533	17.889319	-0.041269	2.596469
210.148629	2157.329849	17.894323	-0.041252	2.592074
210.243069	2149.272125	17.899328	-0.041264	2.587693
210.237217	2141.342640	17.904333	-0.041258	2.583367
210.064907	2133.426791	17.909338	-0.041221	2.579030
210.103095	2125.482201	17.914343	-0.041223	2.574685
210.104791	2117.507230	17.919347	-0.041219	2.570313
209.906709	2109.559103	17.924352	-0.041177	2.565934
209.785332	2101.634524	17.929357	-0.041149	2.561566
209.721054	2093.669037	17.934362	-0.041133	2.557172
209.798053	2085.683826	17.939367	-0.041142	2.552770
209.713712	2077.717026	17.944371	-0.041121	2.548359
209.602837	2069.740971	17.949376	-0.041096	2.543933
209.574429	2061.796465	17.954381	-0.041085	2.539522
209.465241	2053.847453	17.959386	-0.041060	2.535096
209.477059	2045.854916	17.964391	-0.041057	2.530646
209.514093	2037.881026	17.969395	-0.041059	2.526201
209.337460	2029.927582	17.974400	-0.041021	2.521744
209.368408	2021.978105	17.979405	-0.041022	2.517296
209.176910	2014.020341	17.984410	-0.040982	2.512820
209.154816	2006.000934	17.989415	-0.040973	2.508313
209.078544	1998.056411	17.994419	-0.040953	2.503837
209.015102	1990.083818	17.999424	-0.040937	2.499337
209.097096	1982.134979	18.004429	-0.040947	2.494853
209.022383	1974.153131	18.009434	-0.040928	2.490332
209.067977	1966.173523	18.014439	-0.040932	2.485812
208.955478	1958.264896	18.019443	-0.040906	2.481312
208.955826	1950.278427	18.024448	-0.040901	2.476768
208.952770	1942.332495	18.029453	-0.040895	2.472239
208.690622	1934.364993	18.034458	-0.040842	2.467670
208.753477	1926.393945	18.039463	-0.040848	2.463114
208.547601	1918.457237	18.044467	-0.040805	2.458550
208.500540	1910.493944	18.049472	-0.040791	2.453974
208.588504	1902.508568	18.054477	-0.040803	2.449386
208.454169	1894.562422	18.059482	-0.040773	2.444796
208.355957	1886.613830	18.064487	-0.040749	2.440199
208.328317	1878.670703	18.069491	-0.040739	2.435601
208.385309	1870.600932	18.074496	-0.040745	2.430928
208.187008	1862.666833	18.079501	-0.040703	2.426305
208.175945	1854.684334	18.084506	-0.040696	2.421659
208.112884	1846.756675	18.089511	-0.040679	2.417032
208.133508	1838.796544	18.094515	-0.040678	2.412384
208.016801	1830.832681	18.099520	-0.040652	2.407714
208.188950	1822.859714	18.104525	-0.040679	2.403053
208.141089	1814.922932	18.109530	-0.040665	2.398386
207.788263	1807.016898	18.114535	-0.040594	2.393704
207.971054	1799.008413	18.119539	-0.040623	2.388995
207.934683	1791.033849	18.124544	-0.040612	2.384279
207.936611	1783.104702	18.129549	-0.040607	2.379584
207.850070	1775.156289	18.134554	-0.040586	2.374861
207.827173	1767.171635	18.139559	-0.040577	2.370112
207.790724	1759.245387	18.144563	-0.040565	2.365387
207.469992	1751.309317	18.149568	-0.040500	2.360625
207.597665	1743.356028	18.154573	-0.040519	2.355878
207.506137	1735.372861	18.159578	-0.040497	2.351086
207.274441	1727.410199	18.164583	-0.040449	2.346285
207.257241	1719.451990	18.169587	-0.040441	2.341494
207.141071	1711.514459	18.174592	-0.040414	2.336698
207.117115	1703.559329	18.179597	-0.040405	2.331889
207.211893	1695.569420	18.184602	-0.040418	2.327059
207.293419	1687.600917	18.189607	-0.040428	2.322231
207.080093	1679.700472	18.194611	-0.040383	2.317409
207.072289	1671.730141	18.199616	-0.040377	2.312552
207.157216	1663.762827	18.204621	-0.040388	2.307695
206.879409	1655.838267	18.209626	-0.040331	2.302823
206.783546	1647.903376	18.214631	-0.040308	2.297949
206.897471	1639.933426	18.219635	-0.040324	2.293061
206.692711	1631.977171	18.224640	-0.040281	2.288144
206.779593	1624.020409	18.229645	-0.040293	2.283241
206.625802	1616.105080	18.234650	-0.040259	2.278333
206.527040	1608.134130	18.239655	-0.040236	2.273384
206.451796	1600.127882	18.244659	-0.040217	2.268404
206.302009	1592.180146	18.249664	-0.040184	2.263444
206.445180	1584.237730	18.254669	-0.040205	2.258501
206.382696	1576.287323	18.259674	-0.040189	2.253525
206.297290	1568.325102	18.264679	-0.040168	2.248528
206.233171	1560.400000	18.269683	-0.040151	2.243545
206.292634	1552.455213	18.274688	-0.040157	2.238549
206.112678	1544.537854	18.279693	-0.040119	2.233539
206.052426	1536.571056	18.284698	-0.040103	2.228496
206.189576	1528.597344	18.289703	-0.040123	2.223456
206.119806	1520.685139	18.294707	-0.040105	2.218424
205.833356	1512.759662	18.299712	-0.040047	2.213353
205.892483	1504.794593	18.304717	-0.040053	2.208276
205.650605	1496.867059	18.309722	-0.040003	2.203185
205.467176	1488.954132	18.314727	-0.039964	2.198096
205.556611	1480.986367	18.319731	-0.039976	2.192985
205.384124	1473.016071	18.324736	-0.039939	2.187836
205.525786	1465.055374	18.329741	-0.039960	2.182710
205.283293	1457.142487	18.334746	-0.039910	2.177568
205.386071	1449.172448	18.339751	-0.039924	2.172408
205.433374	1441.228668	18.344755	-0.039928	2.167248
205.260289	1433.298082	18.349760	-0.039891	2.162064
205.259304	1425.378054	18.354765	-0.039886	2.156890
205.165957	1417.443067	18.359770	-0.039863	2.151685
204.935454	1409.506341	18.364775	-0.039816	2.146454
204.989342	1401.548599	18.369779	-0.039821	2.141223
205.043236	1393.604100	18.374784	-0.039826	2.135987
204.835490	1385.688788	18.379789	-0.039782	2.130734
204.736120	1377.753081	18.384794	-0.039759	2.125464
204.804153	1369.803373	18.389799	-0.039766	2.120187
204.714222	1361.902723	18.394803	-0.039745	2.114915
204.476230	1353.890075	18.399808	-0.039695	2.109541
204.531457	1345.957808	18.404813	-0.039701	2.104235
204.578007	1338.011904	18.409818	-0.039705	2.098906
204.371529	1330.104981	18.414823	-0.039661	2.093565
204.376652	1322.164999	18.419827	-0.039657	2.088208
204.485054	1314.208684	18.424832	-0.039672	2.082837
204.249236	1306.334626	18.429837	-0.039624	2.077474
204.079095	1298.409121	18.434842	-0.039587	2.072068
204.133648	1290.437304	18.439847	-0.039592	2.066639
204.238178	1282.505521	18.444851	-0.039607	2.061228
204.160340	1274.577934	18.449856	-0.039587	2.055787
204.231096	1266.632579	18.454861	-0.039596	2.050334
204.071429	1258.730778	18.459866	-0.039561	2.044874
204.146424	1250.794490	18.464871	-0.039570	2.039399
203.924093	1242.918223	18.469875	-0.039524	2.033921
203.871981	1234.942189	18.474880	-0.039509	2.028376
203.830519	1227.014835	18.479885	-0.039496	2.022851
203.491809	1219.140103	18.484890	-0.039428	2.017316
203.443785	1211.197488	18.489895	-0.039414	2.011749
203.539870	1203.242433	18.494899	-0.039427	2.006173
203.288331	1195.354074	18.499904	-0.039376	2.000591
203.368283	1187.427208	18.504909	-0.039386	1.995002
203.484510	1179.462043	18.509914	-0.039402	1.989374
203.405674	1171.538894	18.514919	-0.039383	1.983739
203.228592	1163.665192	18.519923	-0.039345	1.978112
203.368319	1155.699946	18.524928	-0.039366	1.972438
203.436670	1147.767924	18.529933	-0.039374	1.966764
203.283765	1139.880309	18.534938	-0.039340	1.961082
202.958907	1132.015232	18.539943	-0.039275	1.955380
203.151625	1123.999918	18.544947	-0.039306	1.949609
203.061535	1116.088686	18.549952	-0.039284	1.943866
202.849360	1108.211087	18.554957	-0.039240	1.938117
202.755464	1100.290664	18.559962	-0.039217	1.932333
202.753138	1092.345667	18.564967	-0.039212	1.926523
202.764762	1084.442262	18.569971	-0.039209	1.920728
202.526888	1076.560546	18.574976	-0.039160	1.914903
202.598113	1068.627262	18.579981	-0.039168	1.909057
202.476841	1060.725031	18.584986	-0.039141	1.903195
202.418426	1052.813329	18.589991	-0.039125	1.897314
202.470747	1044.891770	18.594995	-0.039130	1.891421
202.239811	1036.992635	18.600000	-0.039082	1.885493
202.229518	1029.104656	18.605005	-0.039075	1.879580
202.158795	1021.210262	18.610010	-0.039057	1.873637
202.295544	1013.238594	18.615015	-0.039077	1.867640
202.191973	1005.357737	18.620019	-0.039053	1.861666
202.064178	997.451944	18.625024	-0.039025	1.855650
202.047846	989.545161	18.630029	-0.039017	1.849626
202.040434	981.638672	18.635034	-0.039010	1.843585
201.958824	973.755844	18.640039	-0.038990	1.837532
201.893633	965.875420	18.645043	-0.038973	1.831464
201.785925	957.952551	18.650048	-0.038948	1.825338
201.765181	950.071508	18.655053	-0.038939	1.819233
201.528438	942.196079	18.660058	-0.038890	1.813087
201.712050	934.256360	18.665063	-0.038920	1.806920
201.722462	926.384685	18.670067	-0.038917	1.800764
201.554622	918.508725	18.675072	-0.038881	1.794562
201.591485	910.553749	18.680077	-0.038882	1.788302
201.156331	902.711506	18.685082	-0.038797	1.782050
201.031956	894.834852	18.690087	-0.038768	1.775788
201.287404	886.891275	18.695091	-0.038811	1.769497
201.078367	879.015504	18.700096	-0.038767	1.763180
201.014971	871.157226	18.705101	-0.038751	1.756872
201.085256	863.245280	18.710106	-0.038759	1.750515
201.120252	855.344708	18.715111	-0.038760	1.744140
200.887334	847.529140	18.720115	-0.038712	1.737777
200.524055	839.660533	18.725120	-0.038640	1.731330
200.689023	831.740476	18.730125	-0.038665	1.724884
200.661846	823.878693	18.735130	-0.038655	1.718438
200.492612	816.008139	18.740135	-0.038619	1.711941
200.517445	808.103019	18.745139	-0.038619	1.705417
200.424906	800.236443	18.750144	-0.038597	1.698884
200.391529	792.364413	18.755149	-0.038585	1.692329
200.087570	784.516242	18.760154	-0.038524	1.685733
200.177642	776.628636	18.765159	-0.038536	1.679130
200.338365	768.746269	18.770163	-0.038561	1.672514
200.022332	760.900895	18.775168	-0.038497	1.665840
199.939168	753.061769	18.780173	-0.038477	1.659176
199.951660	745.176049	18.785178	-0.038474	1.652458
199.689342	737.332062	18.790183	-0.038421	1.645711
199.878147	729.454103	18.795187	-0.038451	1.638968
199.750822	721.571036	18.800192	-0.038422	1.632150
199.594092	713.702303	18.805197	-0.038388	1.625311
199.649735	705.841912	18.810202	-0.038394	1.618481
199.744377	697.962148	18.815207	-0.038406	1.611610
199.535883	690.144403	18.820211	-0.038363	1.604721
199.201631	682.343462	18.825216	-0.038295	1.597799
199.345157	674.464205	18.830221	-0.038317	1.590846
199.322215	666.612331	18.835226	-0.038308	1.583863
199.022051	658.810251	18.840231	-0.038247	1.576854
199.066145	650.944993	18.845235	-0.038251	1.569806
199.114421	643.089876	18.850240	-0.038255	1.562737
199.158457	635.259842	18.855245	-0.038258	1.555657
199.094733	627.409116	18.860250	-0.038241	1.548510
199.067269	619.569300	18.865255	-0.038231	1.541346
198.820193	611.786944	18.870259	-0.038181	1.534168
198.762807	603.936720	18.875264	-0.038165	1.526922
198.685501	596.130341	18.880269	-0.038146	1.519679
198.780864	588.284189	18.885274	-0.038159	1.512391
198.553040	580.480259	18.890279	-0.038111	1.505057
198.497260	572.676334	18.895283	-0.038096	1.497714
198.301106	564.858756	18.900288	-0.038055	1.490300
198.266738	557.052746	18.905293	-0.038043	1.482885
198.146126	549.268845	18.910298	-0.038016	1.475440
198.093049	541.388970	18.915303	-0.038001	1.467876
198.093216	533.588901	18.920307	-0.037997	1.460359
197.939473	525.794578	18.925312	-0.037963	1.452783
198.016561	517.971334	18.930317	-0.037973	1.445177
197.924529	510.203112	18.935322	-0.037951	1.437557
197.806794	502.405665	18.940327	-0.037924	1.429863
197.821750	494.616656	18.945331	-0.037922	1.422158
197.656374	486.849168	18.950336	-0.037886	1.414402
197.828372	479.023857	18.955341	-0.037913	1.406602
197.767353	471.264916	18.960346	-0.037897	1.398786
197.555732	463.502434	18.965351	-0.037853	1.390897
197.702679	455.697337	18.970355	-0.037875	1.382981
197.400858	447.968202	18.975360	-0.037814	1.375020
197.205166	440.213046	18.980365	-0.037773	1.367005
197.312283	432.436789	18.985370	-0.037788	1.358972
197.039244	424.706907	18.990375	-0.037733	1.350874
196.938387	416.960084	18.995379	-0.037709	1.342739
196.794011	409.214261	19.000384	-0.037677	1.334548
196.724006	401.462804	19.005389	-0.037659	1.326314
196.626848	393.740582	19.010394	-0.037637	1.318054
196.525649	385.900605	19.015399	-0.037613	1.309615
196.728731	378.097871	19.020403	-0.037646	1.301217
196.495449	370.408793	19.025408	-0.037598	1.292809
196.341498	362.704274	19.030413	-0.037564	1.284342
196.402221	354.983092	19.035418	-0.037571	1.275842
196.181983	347.294633	19.040423	-0.037525	1.267268
196.317998	339.570325	19.045427	-0.037545	1.258662
196.206876	331.870907	19.050432	-0.037520	1.249979
196.164453	324.188145	19.055437	-0.037507	1.241266
195.934495	316.529905	19.060442	-0.037460	1.232484
195.641818	308.860582	19.065447	-0.037400	1.223614
195.803967	301.147025	19.070451	-0.037426	1.214717
195.588486	293.484507	19.075456	-0.037381	1.205739
195.483221	285.844212	19.080461	-0.037357	1.196742
195.399636	278.177820	19.085466	-0.037336	1.187650
195.493664	270.495808	19.090471	-0.037349	1.178505
195.442482	262.856696	19.095475	-0.037335	1.169311
195.411917	255.210275	19.100480	-0.037324	1.160040
195.184683	247.600984	19.105485	-0.037277	1.150698
194.954562	239.978189	19.110490	-0.037230	1.141262
194.875973	232.354841	19.115495	-0.037210	1.131778
194.919216	224.736594	19.120499	-0.037214	1.122248
194.617844	217.174868	19.125504	-0.037153	1.112632
194.493210	209.585716	19.130509	-0.037125	1.102937
194.599021	201.976735	19.135514	-0.037140	1.093180
194.369408	194.422016	19.140519	-0.037092	1.083332
194.284989	186.874065	19.145523	-0.037072	1.073434
194.180714	179.298895	19.150528	-0.037048	1.063404
194.140434	171.752584	19.155533	-0.037036	1.053332
194.017874	164.225736	19.160538	-0.037008	1.043170
193.670552	156.757101	19.165543	-0.036939	1.032933
193.722453	149.221166	19.170547	-0.036944	1.022597
193.496678	141.745177	19.175552	-0.036897	1.012172
193.554224	134.235636	19.180557	-0.036903	1.001660
193.471293	126.752537	19.185562	-0.036883	0.991040
193.254855	119.292424	19.190567	-0.036838	0.980304
192.973492	111.882174	19.195571	-0.036781	0.969505
192.989860	104.423357	19.200576	-0.036780	0.958589
192.699338	97.040146	19.205581	-0.036721	0.947581
192.437505	89.667666	19.210586	-0.036668	0.936466
192.258554	82.283049	19.215591	-0.036630	0.925222
192.050485	74.939266	19.220595	-0.036586	0.913894
191.653903	67.614618	19.225600	-0.036508	0.902402
191.216327	60.561612	19.230605	-0.036422	0.891180