Thu Mar 11 18:33:44 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.351072	-0.017402	0.000000	-0.000020	0.724833

0.260659	-0.119883	0.005005	-0.000003	0.724601
0.305874	-0.126772	0.010010	-0.000012	0.724604
0.444926	-0.151883	0.015014	-0.000038	0.724604
0.399132	-0.145879	0.020019	-0.000030	0.724600
0.177279	-0.103268	0.025024	0.000011	0.724607
0.150716	-0.103241	0.030029	0.000016	0.724598
0.173276	-0.104701	0.035034	0.000011	0.724603
0.249653	-0.119650	0.040038	-0.000003	0.724601
0.165133	-0.106553	0.045043	0.000012	0.724598
0.157332	-0.100135	0.050048	0.000014	0.724608
0.281446	-0.126694	0.055053	-0.000010	0.724600
0.141676	-0.101088	0.060058	0.000016	0.724602
0.102532	-0.093756	0.065062	0.000023	0.724603
0.095713	-0.094851	0.070067	0.000024	0.724599
0.131718	-0.102334	0.075072	0.000017	0.724597
-0.050577	-0.239084	0.080077	0.000051	0.724266
0.124912	-0.268171	0.085082	0.000018	0.724271
0.184236	-0.280961	0.090086	0.000007	0.724267
0.047790	-0.258458	0.095091	0.000032	0.724264
0.211642	-0.284197	0.100096	0.000001	0.724271
0.070740	-0.264609	0.105101	0.000027	0.724261
0.152581	-0.322342	0.110106	0.000012	0.724177
0.146243	-0.433627	0.115110	0.000013	0.723957
0.051870	-0.418057	0.120115	0.000030	0.723955
0.047312	-0.413894	0.125120	0.000031	0.723962
-0.223361	-0.369645	0.130125	0.000081	0.723955
-0.119414	-0.386434	0.135130	0.000061	0.723959
-0.031360	-0.564834	0.140134	0.000045	0.723641
-0.166648	-0.542974	0.145139	0.000069	0.723637
0.043665	-0.575675	0.150144	0.000030	0.723646
-0.014021	-0.569304	0.155149	0.000041	0.723639
0.151122	-0.688023	0.160154	0.000010	0.723465
0.045815	-0.726880	0.165158	0.000029	0.723352
0.196264	-0.757525	0.170163	0.000001	0.723345
0.195638	-0.752235	0.175168	0.000001	0.723356
0.025758	-0.888038	0.180173	0.000032	0.723031
0.091991	-0.907428	0.185178	0.000020	0.723016
0.221757	-0.931603	0.190182	-0.000005	0.723014
-0.105001	-0.966801	0.195187	0.000056	0.722832
-0.054776	-1.039903	0.200192	0.000046	0.722706
-0.257160	-1.008876	0.205197	0.000084	0.722697
-0.266471	-1.062417	0.210202	0.000085	0.722589
-0.297314	-1.165156	0.215206	0.000091	0.722377
-0.344965	-1.158218	0.220211	0.000099	0.722375
-0.188084	-1.219105	0.225216	0.000070	0.722310
-0.203308	-1.333645	0.230221	0.000073	0.722080
-0.130497	-1.344142	0.235226	0.000059	0.722086
-0.418112	-1.368664	0.240230	0.000112	0.721938
-0.555189	-1.439875	0.245235	0.000137	0.721750
-0.463518	-1.451509	0.250240	0.000120	0.721760
-0.681880	-1.518547	0.255245	0.000161	0.721552
-0.617093	-1.583806	0.260250	0.000148	0.721447
-0.694438	-1.570983	0.265254	0.000163	0.721446
-0.643803	-1.733067	0.270259	0.000153	0.721145
-1.104218	-1.657031	0.275264	0.000238	0.721134
-1.212501	-1.675526	0.280269	0.000258	0.721060
-0.784710	-1.839947	0.285274	0.000179	0.720887
-0.940062	-1.812479	0.290278	0.000207	0.720887
-1.821457	-1.784555	0.295283	0.000371	0.720634
-1.748406	-1.840907	0.300288	0.000357	0.720549
-1.389448	-1.912718	0.305293	0.000290	0.720534
-2.241487	-1.915838	0.310298	0.000449	0.720229
-2.593403	-1.852293	0.315302	0.000514	0.720231
-2.553092	-1.880357	0.320307	0.000506	0.720191
-3.089127	-1.928262	0.325312	0.000606	0.719909
-3.170069	-1.918440	0.330317	0.000620	0.719900
-3.459400	-1.865485	0.335322	0.000674	0.719904
-4.046163	-1.907383	0.340326	0.000783	0.719616
-4.364417	-1.858147	0.345331	0.000842	0.719601
-4.127647	-1.895638	0.350336	0.000798	0.719611
-4.334509	-1.933475	0.355341	0.000836	0.719464
-5.244554	-1.867119	0.360346	0.001005	0.719276
-4.788377	-1.948400	0.365350	0.000920	0.719276
-5.338221	-1.853521	0.370355	0.001022	0.719271
-5.349319	-1.925076	0.375360	0.001024	0.719126
-6.248339	-1.850861	0.380365	0.001191	0.718957
-5.908673	-1.909692	0.385370	0.001128	0.718961
-6.055218	-1.881414	0.390374	0.001155	0.718966
-6.429645	-1.818208	0.395379	0.001224	0.718959
-6.276574	-1.996409	0.400384	0.001196	0.718662
-7.153888	-1.848775	0.405389	0.001359	0.718646
-7.592170	-1.768420	0.410394	0.001440	0.718651
-6.940274	-1.883693	0.415398	0.001318	0.718653
-7.090445	-1.860978	0.420403	0.001346	0.718645
-7.417317	-1.944064	0.425408	0.001407	0.718367
-7.816493	-1.878342	0.430413	0.001481	0.718356
-8.010030	-1.842130	0.435418	0.001516	0.718360
-8.046000	-1.835248	0.440422	0.001523	0.718362
-7.925478	-1.859716	0.445427	0.001500	0.718356
-8.122460	-1.943274	0.450432	0.001537	0.718122
-9.328100	-1.780966	0.455437	0.001761	0.718019
-8.949424	-1.846633	0.460442	0.001690	0.718023
-8.545463	-1.918542	0.465446	0.001615	0.718024
-9.211798	-1.801912	0.470451	0.001739	0.718020
-9.152013	-1.809991	0.475456	0.001727	0.718026
-9.204739	-1.885335	0.480461	0.001737	0.717859
-10.013314	-1.816631	0.485466	0.001887	0.717711
-9.691504	-1.873120	0.490470	0.001827	0.717713
-10.149356	-1.794726	0.495475	0.001912	0.717707
-9.576151	-1.891056	0.500480	0.001805	0.717719
-9.872427	-1.845668	0.505485	0.001860	0.717705
-10.188626	-1.816514	0.510490	0.001918	0.717651
-10.562775	-1.882167	0.515494	0.001988	0.717390
-10.648905	-1.870337	0.520499	0.002004	0.717384
-10.946423	-1.813868	0.525504	0.002059	0.717391
-10.961662	-1.815534	0.530509	0.002061	0.717383
-10.843156	-1.834983	0.535514	0.002039	0.717387
-10.943153	-1.815156	0.540518	0.002057	0.717391
-11.131865	-1.826103	0.545523	0.002092	0.717304
-11.428221	-1.878676	0.550528	0.002147	0.717096
-11.723904	-1.831609	0.555533	0.002202	0.717085
-12.067209	-1.767892	0.560538	0.002266	0.717091
-11.461226	-1.874568	0.565542	0.002153	0.717093
-11.756113	-1.826696	0.570547	0.002207	0.717085
-12.123804	-1.756663	0.575552	0.002276	0.717094
-11.988740	-1.823920	0.580557	0.002250	0.717009
-12.381836	-1.878460	0.585562	0.002323	0.716763
-12.425944	-1.869616	0.590566	0.002331	0.716766
-13.269209	-1.723073	0.595571	0.002488	0.716759
-12.576037	-1.843193	0.600576	0.002359	0.716766
-12.662563	-1.832472	0.605581	0.002374	0.716757
-13.004808	-1.769259	0.610586	0.002438	0.716762
-12.590696	-1.863568	0.615590	0.002361	0.716722
-13.450389	-1.849446	0.620595	0.002520	0.716447
-13.469484	-1.842417	0.625600	0.002524	0.716455
-13.708354	-1.802309	0.630605	0.002568	0.716450
-13.568770	-1.825044	0.635610	0.002542	0.716455
-13.664060	-1.808463	0.640614	0.002559	0.716455
-14.069596	-1.740637	0.645619	0.002634	0.716446
-13.448493	-1.846702	0.650624	0.002519	0.716456
-13.935854	-1.901093	0.655629	0.002609	0.716177
-14.928008	-1.745158	0.660634	0.002793	0.716136
-14.395638	-1.838297	0.665638	0.002694	0.716140
-14.440758	-1.833923	0.670643	0.002702	0.716133
-14.561700	-1.807728	0.675648	0.002725	0.716143
-14.835323	-1.763950	0.680653	0.002775	0.716133
-14.353050	-1.846903	0.685658	0.002685	0.716140
-14.493544	-1.907245	0.690662	0.002711	0.715971
-15.951101	-1.691672	0.695667	0.002982	0.715884
-15.213693	-1.820276	0.700672	0.002845	0.715890
-14.976080	-1.866502	0.705677	0.002800	0.715883
-15.320874	-1.803819	0.710682	0.002864	0.715886
-15.153481	-1.830999	0.715686	0.002833	0.715892
-15.211979	-1.825539	0.720691	0.002843	0.715882
-15.688197	-1.893880	0.725696	0.002932	0.715579
-16.428660	-1.777206	0.730701	0.003069	0.715549
-16.502836	-1.761983	0.735706	0.003083	0.715554
-16.102577	-1.832971	0.740710	0.003008	0.715555
-16.564157	-1.755152	0.745715	0.003094	0.715547
-16.115477	-1.830513	0.750720	0.003010	0.715556
-16.215521	-1.816115	0.755725	0.003029	0.715550
-17.026367	-1.789823	0.760730	0.003179	0.715316
-17.379375	-1.765380	0.765734	0.003245	0.715240
-16.912125	-1.852593	0.770739	0.003158	0.715233
-16.982229	-1.835932	0.775744	0.003170	0.715241
-17.571685	-1.735171	0.780749	0.003280	0.715233
-17.197176	-1.800157	0.785754	0.003210	0.715237
-16.704477	-1.885804	0.790758	0.003118	0.715242
-17.440862	-1.853526	0.795763	0.003255	0.715046
-18.351724	-1.756981	0.800768	0.003424	0.714916
-17.809368	-1.857023	0.805773	0.003323	0.714910
-17.947856	-1.832036	0.810778	0.003348	0.714911
-17.912284	-1.836209	0.815782	0.003342	0.714916
-18.122153	-1.802635	0.820787	0.003380	0.714909
-18.030538	-1.814944	0.825792	0.003363	0.714917
-18.236859	-1.845670	0.830797	0.003401	0.714784
-19.117941	-1.772997	0.835802	0.003565	0.714617
-18.684559	-1.849026	0.840806	0.003484	0.714620
-19.210637	-1.759666	0.845811	0.003582	0.714611
-18.976442	-1.797929	0.850816	0.003538	0.714619
-18.520523	-1.883988	0.855821	0.003453	0.714610
-19.131890	-1.775187	0.860826	0.003566	0.714610
-19.018772	-1.853280	0.865830	0.003545	0.714495
-19.799093	-1.824415	0.870835	0.003690	0.714277
-19.433710	-1.884913	0.875840	0.003622	0.714287
-20.104805	-1.768848	0.880845	0.003747	0.714280
-19.839326	-1.815320	0.885850	0.003697	0.714282
-19.310401	-1.907588	0.890854	0.003598	0.714287
-20.293611	-1.736624	0.895859	0.003781	0.714279
-20.026167	-1.838530	0.900864	0.003731	0.714171
-20.392973	-1.873542	0.905869	0.003799	0.713972
-20.330423	-1.884489	0.910874	0.003787	0.713973
-20.841577	-1.790828	0.915878	0.003882	0.713979
-20.924167	-1.781926	0.920883	0.003897	0.713968
-20.446546	-1.863328	0.925888	0.003808	0.713976
-20.770511	-1.807494	0.930893	0.003868	0.713972
-20.616705	-1.912378	0.935898	0.003839	0.713819
-21.294409	-1.871807	0.940902	0.003965	0.713660
-21.677746	-1.809437	0.945907	0.004036	0.713649
-21.632908	-1.814285	0.950912	0.004028	0.713655
-21.479541	-1.844279	0.955917	0.003999	0.713651
-21.538523	-1.833417	0.960922	0.004010	0.713652
-21.603238	-1.817451	0.965926	0.004021	0.713661
-21.577298	-1.900067	0.970931	0.004016	0.713506
-22.318776	-1.835969	0.975936	0.004154	0.713372
-22.435362	-1.820259	0.980941	0.004176	0.713362
-22.814885	-1.753031	0.985946	0.004246	0.713362
-22.248733	-1.850528	0.990950	0.004140	0.713369
-22.562807	-1.799788	0.995955	0.004199	0.713359
-22.507224	-1.806631	1.000960	0.004188	0.713365
-22.243217	-1.921077	1.005965	0.004139	0.713232
-23.244698	-1.847454	1.010970	0.004325	0.713024
-23.259383	-1.841778	1.015974	0.004327	0.713030
-23.796187	-1.751350	1.020979	0.004427	0.713020
-23.324326	-1.829972	1.025984	0.004339	0.713032
-23.124007	-1.869703	1.030989	0.004301	0.713024
-23.592837	-1.785660	1.035994	0.004388	0.713026
-23.271284	-1.886367	1.040998	0.004328	0.712940
-24.532305	-1.778054	1.046003	0.004563	0.712709
-24.381172	-1.802082	1.051008	0.004535	0.712715
-24.506624	-1.782473	1.056013	0.004558	0.712710
-24.525266	-1.778446	1.061018	0.004561	0.712712
-24.406968	-1.796427	1.066022	0.004539	0.712718
-24.622465	-1.763127	1.071027	0.004578	0.712709
-24.204354	-1.833509	1.076032	0.004500	0.712717
-24.590728	-1.847491	1.081037	0.004572	0.712553
-25.844962	-1.707010	1.086042	0.004805	0.712388
-24.818587	-1.885739	1.091046	0.004614	0.712397
-25.352387	-1.795641	1.096051	0.004713	0.712387
-25.757749	-1.717849	1.101056	0.004788	0.712399
-25.203659	-1.819752	1.106061	0.004685	0.712393
-25.179228	-1.824027	1.111066	0.004680	0.712394
-25.332095	-1.795496	1.116070	0.004708	0.712397
-26.111255	-1.808192	1.121075	0.004853	0.712095
-25.964738	-1.831793	1.126080	0.004826	0.712101
-26.164819	-1.799236	1.131085	0.004863	0.712095
-26.151958	-1.801567	1.136090	0.004860	0.712095
-25.944532	-1.837588	1.141094	0.004821	0.712098
-26.414966	-1.758385	1.146099	0.004909	0.712089
-26.192289	-1.792659	1.151104	0.004867	0.712100
-26.559312	-1.860207	1.156109	0.004935	0.711836
-27.192385	-1.782869	1.161114	0.005053	0.711765
-27.099795	-1.794945	1.166118	0.005035	0.711775
-26.936871	-1.828870	1.171123	0.005004	0.711765
-26.776454	-1.852092	1.176128	0.004974	0.711777
-26.836138	-1.846273	1.181133	0.004985	0.711767
-27.399534	-1.746430	1.186138	0.005090	0.711767
-27.011625	-1.923583	1.191142	0.005017	0.711552
-27.995583	-1.795482	1.196147	0.005200	0.711458
-28.028727	-1.785507	1.201152	0.005206	0.711467
-27.922101	-1.807052	1.206157	0.005186	0.711462
-28.016043	-1.792073	1.211162	0.005203	0.711459
-27.872591	-1.816423	1.216166	0.005177	0.711462
-28.147269	-1.770451	1.221171	0.005227	0.711456
-28.034565	-1.893197	1.226176	0.005206	0.711252
-28.883274	-1.796878	1.231181	0.005364	0.711143
-29.087721	-1.761150	1.236186	0.005402	0.711142
-28.795900	-1.811119	1.241190	0.005347	0.711147
-28.979552	-1.783009	1.246195	0.005381	0.711138
-28.857651	-1.800234	1.251200	0.005358	0.711147
-28.770713	-1.819794	1.256205	0.005342	0.711140
-29.084502	-1.823519	1.261210	0.005400	0.711021
-29.764505	-1.774287	1.266214	0.005526	0.710878
-29.723155	-1.786622	1.271219	0.005518	0.710869
-29.495798	-1.823815	1.276224	0.005476	0.710876
-29.531604	-1.819585	1.281229	0.005482	0.710872
-29.781958	-1.775168	1.286234	0.005529	0.710872
-29.630555	-1.799804	1.291238	0.005500	0.710877
-29.569205	-1.903110	1.296243	0.005489	0.710693
-30.743043	-1.770723	1.301248	0.005707	0.710540
-30.766742	-1.768611	1.306253	0.005711	0.710536
-30.480243	-1.821465	1.311258	0.005657	0.710533
-30.516265	-1.815281	1.316262	0.005664	0.710533
-30.696879	-1.785870	1.321267	0.005697	0.710528
-30.510805	-1.815240	1.326272	0.005662	0.710536
-30.255719	-1.938141	1.331277	0.005615	0.710382
-31.713982	-1.761199	1.336282	0.005886	0.710217
-31.345588	-1.823140	1.341286	0.005817	0.710225
-31.324727	-1.831858	1.346291	0.005813	0.710215
-31.388316	-1.818574	1.351296	0.005824	0.710220
-31.434360	-1.812128	1.356301	0.005833	0.710216
-31.462239	-1.805832	1.361306	0.005838	0.710220
-31.628838	-1.864756	1.366310	0.005869	0.710043
-32.913401	-1.710874	1.371315	0.006107	0.709893
-32.160704	-1.841854	1.376320	0.005967	0.709900
-31.941678	-1.882997	1.381325	0.005926	0.709896
-32.724206	-1.744829	1.386330	0.006071	0.709894
-32.297294	-1.818023	1.391334	0.005992	0.709901
-32.046903	-1.868230	1.396339	0.005945	0.709890
-32.352512	-1.885593	1.401344	0.006002	0.709747
-33.684200	-1.721246	1.406349	0.006249	0.709601
-33.358159	-1.780251	1.411354	0.006188	0.709600
-33.020537	-1.837808	1.416358	0.006125	0.709606
-33.379183	-1.778926	1.421363	0.006192	0.709596
-33.405419	-1.771481	1.426368	0.006196	0.709602
-33.241151	-1.801890	1.431373	0.006166	0.709600
-33.490550	-1.762946	1.436378	0.006212	0.709590
-33.766184	-1.871281	1.441382	0.006263	0.709275
-34.071281	-1.821627	1.446387	0.006319	0.709266
-34.162743	-1.804119	1.451392	0.006336	0.709269
-34.236454	-1.789034	1.456397	0.006350	0.709273
-34.084934	-1.818847	1.461402	0.006321	0.709268
-33.989513	-1.833359	1.466406	0.006303	0.709274
-34.384993	-1.768103	1.471411	0.006377	0.709264
-34.793327	-1.844291	1.476416	0.006452	0.708966
-34.720876	-1.859427	1.481421	0.006439	0.708962
-35.341929	-1.752562	1.486426	0.006554	0.708955
-35.283888	-1.757956	1.491430	0.006543	0.708965
-35.111356	-1.792723	1.496435	0.006511	0.708958
-35.037228	-1.803324	1.501440	0.006497	0.708963
-35.223136	-1.772414	1.506445	0.006531	0.708959
-35.095337	-1.908507	1.511450	0.006507	0.708733
-35.701561	-1.843096	1.516454	0.006620	0.708648
-35.732354	-1.842246	1.521459	0.006625	0.708639
-35.866525	-1.815724	1.526464	0.006650	0.708645
-35.893786	-1.811841	1.531469	0.006655	0.708644
-35.950284	-1.803293	1.536474	0.006665	0.708641
-35.819055	-1.827541	1.541478	0.006640	0.708640
-36.590284	-1.835637	1.546483	0.006784	0.708349
-36.626636	-1.826822	1.551488	0.006790	0.708354
-37.030245	-1.756913	1.556493	0.006865	0.708350
-36.952890	-1.771520	1.561498	0.006850	0.708349
-36.601197	-1.830700	1.566502	0.006785	0.708356
-37.170378	-1.733890	1.571507	0.006890	0.708348
-36.856866	-1.786537	1.576512	0.006832	0.708355
-36.630025	-1.944115	1.581517	0.006789	0.708120
-38.098483	-1.738800	1.586522	0.007062	0.708008
-38.103812	-1.731311	1.591526	0.007063	0.708021
-37.881083	-1.775761	1.596531	0.007021	0.708012
-37.572548	-1.827680	1.601536	0.006964	0.708019
-37.639892	-1.818326	1.606541	0.006976	0.708014
-37.665643	-1.814673	1.611546	0.006981	0.708013
-37.394285	-1.948369	1.616550	0.006930	0.707842
-38.575243	-1.810458	1.621555	0.007149	0.707697
-38.490365	-1.821697	1.626560	0.007133	0.707705
-38.269251	-1.864185	1.631565	0.007092	0.707699
-38.461210	-1.829505	1.636570	0.007127	0.707701
-38.257161	-1.862842	1.641574	0.007089	0.707707
-38.245580	-1.889540	1.646579	0.007087	0.707658
-39.054740	-1.882838	1.651584	0.007237	0.707383
-39.103876	-1.875443	1.656589	0.007246	0.707381
-39.523626	-1.804478	1.661594	0.007324	0.707374
-38.837019	-1.921185	1.666598	0.007196	0.707385
-39.187224	-1.862849	1.671603	0.007261	0.707378
-39.429992	-1.817090	1.676608	0.007306	0.707383
-39.085163	-1.960577	1.681613	0.007242	0.707219
-40.340032	-1.806034	1.686618	0.007475	0.707081
-40.456684	-1.781938	1.691622	0.007496	0.707088
-40.526107	-1.773454	1.696627	0.007509	0.707080
-40.208669	-1.826928	1.701632	0.007450	0.707087
-40.037702	-1.859310	1.706637	0.007418	0.707084
-40.572003	-1.765163	1.711642	0.007517	0.707082
-40.215987	-1.882583	1.716646	0.007450	0.706974
-41.018468	-1.850231	1.721651	0.007599	0.706752
-41.126236	-1.827720	1.726656	0.007619	0.706759
-41.377255	-1.784104	1.731661	0.007666	0.706758
-41.365283	-1.788067	1.736666	0.007663	0.706755
-40.939124	-1.860536	1.741670	0.007584	0.706762
-41.439477	-1.776517	1.746675	0.007677	0.706752
-41.137734	-1.847054	1.751680	0.007620	0.706719
-41.674913	-1.886303	1.756685	0.007720	0.706448
-42.252429	-1.785535	1.761690	0.007827	0.706444
-42.077520	-1.811666	1.766694	0.007794	0.706455
-41.840166	-1.860737	1.771699	0.007750	0.706442
-42.225540	-1.787267	1.776704	0.007821	0.706452
-42.334869	-1.768013	1.781709	0.007842	0.706452
-42.006456	-1.830286	1.786714	0.007780	0.706445
-42.384276	-1.899478	1.791718	0.007850	0.706171
-43.489256	-1.725878	1.796723	0.008056	0.706124
-43.092170	-1.793016	1.801728	0.007982	0.706132
-42.541047	-1.891922	1.806733	0.007879	0.706131
-43.564738	-1.711460	1.811738	0.008069	0.706128
-42.858351	-1.834782	1.816742	0.007937	0.706133
-42.777499	-1.853002	1.821747	0.007922	0.706126
-43.380708	-1.821017	1.826752	0.008034	0.705975
-43.919905	-1.780322	1.831757	0.008134	0.705864
-43.602806	-1.838754	1.836762	0.008075	0.705860
-43.496849	-1.854385	1.841766	0.008055	0.705867
-44.151494	-1.743121	1.846771	0.008177	0.705857
-43.754816	-1.809684	1.851776	0.008103	0.705866
-43.590761	-1.837380	1.856781	0.008072	0.705869
-44.389759	-1.821517	1.861786	0.008220	0.705615
-44.673591	-1.811691	1.866790	0.008273	0.705534
-44.680501	-1.816590	1.871795	0.008274	0.705522
-44.718503	-1.806328	1.876800	0.008281	0.705529
-44.884481	-1.778953	1.881805	0.008311	0.705525
-44.503770	-1.847677	1.886810	0.008240	0.705524
-44.515358	-1.841774	1.891814	0.008242	0.705532
-45.065266	-1.850087	1.896819	0.008344	0.705319
-45.667788	-1.794324	1.901824	0.008456	0.705215
-45.118085	-1.893797	1.906829	0.008354	0.705213
-45.898365	-1.757024	1.911834	0.008499	0.705209
-45.922125	-1.748487	1.916838	0.008503	0.705218
-45.633038	-1.804407	1.921843	0.008449	0.705209
-45.514243	-1.823068	1.926848	0.008426	0.705215
-45.953091	-1.820662	1.931853	0.008508	0.705063
-46.786146	-1.759083	1.936858	0.008663	0.704888
-45.965398	-1.903584	1.941862	0.008510	0.704892
-46.653789	-1.782995	1.946867	0.008638	0.704888
-46.578311	-1.795795	1.951872	0.008623	0.704890
-46.110876	-1.879712	1.956877	0.008536	0.704889
-46.627303	-1.789625	1.961882	0.008632	0.704886
-46.566087	-1.872224	1.966886	0.008620	0.704742
-47.560931	-1.770176	1.971891	0.008805	0.704591
-47.313103	-1.813083	1.976896	0.008759	0.704594
-47.635395	-1.754272	1.981901	0.008819	0.704597
-47.527934	-1.776726	1.986906	0.008798	0.704591
-47.086397	-1.852115	1.991910	0.008716	0.704598
-47.707843	-1.745006	1.996915	0.008831	0.704591
-47.615967	-1.846636	2.001920	0.008814	0.704420

-48.389573	-1.786996	2.011917	0.008958	0.704263
-48.025513	-1.853186	2.021914	0.008889	0.704261
-48.387064	-1.789276	2.031910	0.008956	0.704261
-48.294854	-1.806108	2.041907	0.008939	0.704261
-48.364168	-1.792709	2.051904	0.008951	0.704264
-48.379627	-1.790152	2.061901	0.008953	0.704265
-48.176625	-1.828016	2.071898	0.008915	0.704262
-48.348130	-1.797561	2.081894	0.008946	0.704263
-47.911171	-1.873492	2.091891	0.008865	0.704268
-48.133936	-1.834479	2.101888	0.008906	0.704268
-48.346046	-1.778294	2.111885	0.008945	0.704306
-47.295992	-1.823391	2.121882	0.008749	0.704593
-47.507783	-1.786064	2.131878	0.008788	0.704593
-46.941447	-1.886880	2.141875	0.008682	0.704594
-47.130631	-1.852964	2.151872	0.008716	0.704596
-47.306498	-1.819986	2.161869	0.008749	0.704600
-47.301921	-1.814989	2.171866	0.008747	0.704613
-46.809190	-1.764345	2.181862	0.008655	0.704892
-46.358278	-1.845280	2.191859	0.008571	0.704892
-46.534323	-1.813279	2.201856	0.008603	0.704894
-46.511372	-1.818928	2.211853	0.008598	0.704892
-45.878804	-1.792998	2.221850	0.008480	0.705173
-45.856590	-1.779339	2.231846	0.008475	0.705209
-45.370265	-1.864916	2.241843	0.008384	0.705212
-45.723282	-1.801211	2.251840	0.008449	0.705215
-44.853276	-1.808375	2.261837	0.008287	0.705513
-44.820687	-1.808635	2.271834	0.008280	0.705525
-44.758513	-1.819840	2.281830	0.008268	0.705526
-44.866930	-1.759385	2.291827	0.008288	0.705610
-43.907325	-1.804075	2.301824	0.008109	0.705865
-43.534311	-1.871079	2.311821	0.008039	0.705865
-43.962242	-1.797635	2.321818	0.008118	0.705860
-43.773969	-1.770112	2.331814	0.008082	0.705984
-42.997162	-1.836917	2.341811	0.007937	0.706129
-43.129565	-1.812891	2.351808	0.007962	0.706131
-43.213223	-1.785271	2.361805	0.007977	0.706157
-42.511476	-1.768446	2.371802	0.007845	0.706443
-42.147031	-1.833376	2.381798	0.007777	0.706444
-42.182584	-1.826614	2.391795	0.007783	0.706446
-41.708753	-1.813644	2.401792	0.007695	0.706643
-41.213058	-1.845399	2.411789	0.007602	0.706758
-41.469747	-1.802059	2.421786	0.007649	0.706754
-41.218604	-1.836091	2.431782	0.007602	0.706776
-40.668581	-1.781224	2.441779	0.007499	0.707084
-40.492753	-1.813424	2.451776	0.007466	0.707083
-40.329959	-1.841589	2.461773	0.007435	0.707086
-40.035817	-1.809772	2.471770	0.007380	0.707256
-39.561326	-1.833330	2.481766	0.007291	0.707380
-39.343740	-1.872973	2.491763	0.007250	0.707379
-39.559485	-1.834131	2.501760	0.007289	0.707380
-38.705705	-1.832135	2.511757	0.007130	0.707691
-38.912127	-1.791487	2.521754	0.007168	0.707699
-38.527361	-1.861396	2.531750	0.007096	0.707698
-38.625220	-1.760721	2.541747	0.007113	0.707866
-37.710211	-1.849873	2.551744	0.006943	0.708015
-38.030085	-1.793486	2.561741	0.007002	0.708014
-37.962851	-1.785045	2.571738	0.006989	0.708056
-37.028474	-1.805599	2.581734	0.006814	0.708350
-36.684295	-1.866243	2.591731	0.006750	0.708352
-37.053519	-1.801101	2.601728	0.006818	0.708352
-36.575744	-1.794593	2.611725	0.006728	0.708536
-36.338333	-1.786503	2.621722	0.006684	0.708638
-36.149055	-1.820318	2.631718	0.006648	0.708639
-36.331875	-1.738492	2.641715	0.006682	0.708739
-35.185546	-1.832504	2.651712	0.006468	0.708960
-35.162619	-1.836943	2.661709	0.006463	0.708961
-35.345208	-1.806979	2.671706	0.006496	0.708956
-34.558166	-1.815245	2.681702	0.006349	0.709222
-34.548950	-1.793926	2.691699	0.006347	0.709269
-34.329305	-1.835260	2.701696	0.006306	0.709265
-34.086876	-1.809765	2.711693	0.006260	0.709403
-33.281842	-1.858345	2.721690	0.006110	0.709594
-33.270402	-1.859916	2.731686	0.006107	0.709596
-33.366190	-1.842885	2.741683	0.006124	0.709597
-33.008628	-1.828924	2.751680	0.006057	0.709753
-32.753959	-1.803331	2.761677	0.006009	0.709896
-32.783873	-1.798392	2.771674	0.006015	0.709896
-32.460955	-1.830024	2.781670	0.005954	0.709949
-31.717649	-1.827670	2.791667	0.005815	0.710219
-31.667335	-1.837146	2.801664	0.005805	0.710219
-31.868257	-1.800598	2.811661	0.005842	0.710222
-31.159041	-1.819186	2.821658	0.005710	0.710438
-30.865133	-1.825162	2.831654	0.005654	0.710532
-30.895857	-1.818318	2.841651	0.005660	0.710535
-30.539578	-1.857511	2.851648	0.005593	0.710585
-30.038151	-1.803269	2.861645	0.005499	0.710873
-29.882027	-1.831483	2.871642	0.005469	0.710873
-29.878026	-1.832470	2.881638	0.005468	0.710873
-29.707082	-1.783496	2.891635	0.005436	0.711033
-29.129163	-1.832089	2.901632	0.005328	0.711142
-29.318780	-1.799005	2.911629	0.005362	0.711142
-29.217092	-1.774358	2.921626	0.005343	0.711228
-28.463082	-1.794882	2.931622	0.005202	0.711456
-28.436706	-1.801071	2.941619	0.005197	0.711454
-28.135068	-1.851765	2.951616	0.005140	0.711461
-27.896372	-1.745538	2.961613	0.005095	0.711759
-27.385996	-1.838128	2.971610	0.005000	0.711756
-27.560800	-1.806078	2.981606	0.005032	0.711759
-27.119939	-1.765218	2.991603	0.004949	0.711998
-26.400999	-1.847836	3.001600	0.004815	0.712090
-26.634276	-1.806974	3.011597	0.004858	0.712089
-26.528399	-1.800309	3.021594	0.004837	0.712141
-25.875802	-1.794832	3.031590	0.004715	0.712384
-25.582488	-1.846623	3.041587	0.004660	0.712386
-25.615482	-1.841372	3.051584	0.004666	0.712386
-25.309020	-1.780532	3.061581	0.004608	0.712617
-24.697490	-1.844238	3.071578	0.004494	0.712708
-25.022620	-1.785638	3.081574	0.004554	0.712710
-24.727810	-1.798441	3.091571	0.004499	0.712790
-23.965068	-1.816197	3.101568	0.004356	0.713026
-24.078613	-1.796829	3.111565	0.004377	0.713025
-24.099371	-1.794936	3.121562	0.004380	0.713023
-23.610646	-1.732399	3.131558	0.004289	0.713321
-23.132492	-1.797711	3.141555	0.004199	0.713362
-22.918654	-1.834827	3.151552	0.004159	0.713365
-22.872038	-1.794722	3.161549	0.004150	0.713462
-22.030487	-1.850531	3.171546	0.003993	0.713650
-22.285215	-1.805263	3.181542	0.004040	0.713651
-22.130581	-1.832695	3.191539	0.004010	0.713652
-21.586421	-1.809225	3.201536	0.003908	0.713892
-21.685245	-1.753513	3.211533	0.003926	0.713969
-21.072387	-1.864430	3.221530	0.003812	0.713966
-21.404055	-1.759599	3.231526	0.003873	0.714058
-20.292643	-1.848605	3.241523	0.003666	0.714276
-20.539004	-1.804004	3.251520	0.003711	0.714278
-20.291977	-1.849900	3.261517	0.003665	0.714275
-19.964829	-1.779349	3.271514	0.003603	0.714532
-19.686011	-1.790959	3.281510	0.003551	0.714609
-19.305229	-1.859031	3.291507	0.003479	0.714609
-19.442869	-1.804473	3.301504	0.003504	0.714670
-18.642558	-1.827435	3.311501	0.003355	0.714908
-18.497888	-1.854150	3.321498	0.003328	0.714907
-18.814630	-1.799216	3.331494	0.003386	0.714905
-18.019392	-1.844038	3.341491	0.003237	0.715098
-17.804284	-1.814677	3.351488	0.003197	0.715233
-17.495343	-1.871957	3.361485	0.003139	0.715230
-17.801473	-1.818442	3.371482	0.003195	0.715229
-17.099129	-1.794405	3.381478	0.003064	0.715525
-16.739521	-1.848295	3.391475	0.002997	0.715547
-16.771155	-1.842538	3.401472	0.003002	0.715548
-16.685101	-1.793453	3.411469	0.002986	0.715676
-15.600665	-1.883680	3.421466	0.002783	0.715881
-16.009543	-1.810761	3.431462	0.002859	0.715882
-15.571514	-1.888906	3.441459	0.002777	0.715883
-15.557979	-1.820913	3.451456	0.002774	0.716024
-14.825114	-1.894577	3.461453	0.002637	0.716137
-15.203250	-1.829423	3.471450	0.002707	0.716134
-15.069132	-1.834059	3.481446	0.002681	0.716173
-14.044248	-1.878075	3.491443	0.002490	0.716448
-14.324270	-1.828664	3.501440	0.002542	0.716448
-13.994537	-1.887199	3.511437	0.002480	0.716449
-13.762932	-1.835529	3.521434	0.002436	0.716634
-13.526446	-1.817598	3.531430	0.002391	0.716754
-13.519574	-1.818383	3.541427	0.002390	0.716756
-13.470764	-1.768590	3.551424	0.002380	0.716873
-12.392715	-1.853295	3.561421	0.002179	0.717086
-12.794772	-1.782979	3.571418	0.002253	0.717084
-12.422669	-1.848267	3.581414	0.002184	0.717087
-12.010203	-1.773674	3.591411	0.002106	0.717381
-11.723213	-1.824512	3.601408	0.002052	0.717382
-11.524841	-1.861541	3.611405	0.002015	0.717380
-11.296915	-1.794973	3.621402	0.001972	0.717593
-10.710638	-1.845821	3.631398	0.001862	0.717700
-10.783170	-1.832146	3.641395	0.001875	0.717702
-10.570014	-1.862911	3.651392	0.001835	0.717717
-10.110304	-1.793032	3.661389	0.001749	0.718018
-9.987304	-1.815845	3.671386	0.001726	0.718017
-9.807634	-1.849622	3.681382	0.001692	0.718015
-9.457472	-1.807335	3.691379	0.001626	0.718222
-8.865958	-1.845882	3.701376	0.001515	0.718355
-8.799042	-1.856924	3.711373	0.001502	0.718358
-9.129966	-1.795446	3.721370	0.001564	0.718364
-8.109554	-1.837202	3.731366	0.001373	0.718641
-7.973668	-1.859261	3.741363	0.001347	0.718646
-7.929403	-1.866070	3.751360	0.001339	0.718649
-8.151575	-1.757830	3.761357	0.001379	0.718786
-7.127082	-1.851605	3.771354	0.001188	0.718962
-7.153236	-1.846902	3.781350	0.001193	0.718963
-7.148631	-1.847399	3.791347	0.001191	0.718964
-6.676470	-1.791937	3.801344	0.001103	0.719240
-6.197421	-1.861990	3.811341	0.001013	0.719271
-6.386889	-1.830659	3.821338	0.001048	0.719268
-6.174759	-1.797802	3.831334	0.001008	0.719408
-5.483540	-1.821190	3.841331	0.000879	0.719605
-5.332734	-1.846733	3.851328	0.000850	0.719609
-5.411635	-1.832636	3.861325	0.000864	0.719610
-4.604208	-1.845392	3.871322	0.000713	0.719869
-4.494634	-1.850659	3.881318	0.000693	0.719898
-4.384691	-1.869558	3.891315	0.000672	0.719900
-4.339126	-1.849144	3.901312	0.000663	0.719957
-3.722129	-1.823155	3.911309	0.000547	0.720226
-3.721372	-1.823601	3.921306	0.000547	0.720226
-3.587678	-1.848158	3.931302	0.000521	0.720226
-3.352539	-1.781545	3.941299	0.000477	0.720440
-2.910652	-1.806950	3.951296	0.000394	0.720546
-2.809328	-1.825781	3.961293	0.000375	0.720545
-2.813644	-1.765681	3.971290	0.000375	0.720663
-2.262509	-1.751854	3.981286	0.000272	0.720884
-2.087816	-1.782796	3.991283	0.000239	0.720885
-2.144477	-1.752956	4.001280	0.000249	0.720925
-1.816728	-1.709160	4.011277	0.000187	0.721127
-1.757703	-1.719942	4.021274	0.000176	0.721127
-1.857608	-1.640108	4.031270	0.000194	0.721250
-1.139202	-1.670161	4.041267	0.000060	0.721444
-1.473532	-1.610024	4.051264	0.000122	0.721446
-1.084452	-1.553647	4.061261	0.000049	0.721694
-1.491173	-1.453655	4.071258	0.000124	0.721749
-1.142771	-1.414528	4.081254	0.000058	0.721949
-0.869645	-1.395515	4.091251	0.000007	0.722082
-0.673063	-1.356649	4.101248	-0.000030	0.722228
-0.671762	-1.280767	4.111245	-0.000031	0.722379
-0.723120	-1.185021	4.121242	-0.000022	0.722550
-0.704493	-1.112827	4.131238	-0.000026	0.722699
-0.748341	-0.977985	4.141235	-0.000018	0.722949
-0.660549	-0.924998	4.151232	-0.000035	0.723084
-0.571648	-0.806787	4.161229	-0.000052	0.723348
-0.605471	-0.698337	4.171226	-0.000047	0.723550
-0.582792	-0.608253	4.181222	-0.000051	0.723735
-0.450139	-0.518057	4.191219	-0.000077	0.723959
-0.143210	-0.421257	4.201216	-0.000134	0.724257
-0.201661	-0.300986	4.211213	-0.000124	0.724473
-0.010728	-0.220847	4.221210	-0.000160	0.724697
-0.081187	-0.092140	4.231206	-0.000148	0.724925
-0.056943	0.055592	4.241203	-0.000153	0.725223
0.000000	0.225573	4.251200	-0.000164	0.725576

-0.154330	0.868544	4.256205	-0.000136	0.726779
0.292287	2.065690	4.261210	-0.000220	0.729266
0.591730	3.878051	4.266214	-0.000277	0.732885
0.954495	6.233531	4.271219	-0.000346	0.737554
1.311080	9.106971	4.276224	-0.000415	0.743179
1.771495	12.446073	4.281229	-0.000503	0.749679
2.400466	16.209486	4.286234	-0.000623	0.756974
2.796498	20.421158	4.291238	-0.000700	0.764953
3.418968	24.995895	4.296243	-0.000819	0.773590
4.242740	29.913797	4.301248	-0.000976	0.782818
5.020351	35.191857	4.306253	-0.001124	0.792568
6.006403	40.752605	4.311258	-0.001312	0.802763
7.264124	46.597628	4.316262	-0.001550	0.813410
8.236483	52.756435	4.321267	-0.001735	0.824371
9.287600	59.196955	4.326272	-0.001935	0.835690
10.199445	65.857025	4.331277	-0.002110	0.847183
10.781399	72.813152	4.336282	-0.002223	0.858915
11.556775	79.946032	4.341286	-0.002372	0.870832
12.393800	87.236805	4.346291	-0.002533	0.882858
13.176914	94.733888	4.351296	-0.002684	0.895034
13.707207	102.423125	4.356301	-0.002788	0.907277
14.327119	110.237074	4.361306	-0.002909	0.919573
15.392099	118.087586	4.366310	-0.003112	0.931881
16.059706	126.120192	4.371315	-0.003242	0.944197
16.680581	134.276034	4.376320	-0.003363	0.956524
17.674966	142.444441	4.381325	-0.003554	0.968808
18.641169	150.696048	4.386330	-0.003740	0.981050
19.306705	159.123268	4.391334	-0.003869	0.993317
19.978699	167.546518	4.396339	-0.004000	1.005430
20.902775	175.993703	4.401344	-0.004178	1.017492
21.451727	184.532603	4.406349	-0.004286	1.029450
21.845340	193.127112	4.411354	-0.004365	1.041308
22.558528	201.699078	4.416358	-0.004504	1.053077
23.352506	210.267105	4.421363	-0.004657	1.064729
23.848859	218.938736	4.426368	-0.004756	1.076324
24.536918	227.543936	4.431373	-0.004890	1.087750
25.340787	236.159095	4.436378	-0.005045	1.099096
26.165397	244.787269	4.441382	-0.005205	1.110347
27.022376	253.385727	4.446387	-0.005370	1.121454
27.904512	262.017398	4.451392	-0.005540	1.132499
28.970972	270.592911	4.456397	-0.005745	1.143406
30.204156	279.192514	4.461402	-0.005980	1.154274
31.153718	287.793518	4.466406	-0.006163	1.164983
31.739979	296.452291	4.471411	-0.006278	1.175588
32.172153	305.117083	4.476416	-0.006364	1.186075
32.746565	313.750096	4.481421	-0.006477	1.196460
33.790065	322.273321	4.486426	-0.006677	1.206720
34.203501	330.924986	4.491430	-0.006760	1.216918
34.577569	339.532008	4.496435	-0.006835	1.226972
35.561481	348.054370	4.501440	-0.007024	1.236965
36.404812	356.548007	4.506445	-0.007187	1.246818
36.756808	365.140989	4.511450	-0.007259	1.256612
37.336407	373.662730	4.516454	-0.007372	1.266293
38.202423	382.136360	4.521459	-0.007539	1.275901
39.214854	390.569058	4.526464	-0.007734	1.285418
39.656602	399.095152	4.531469	-0.007822	1.294863
40.050429	407.607949	4.536474	-0.007901	1.304215
40.913260	416.140432	4.541478	-0.008067	1.313607
41.550127	424.575248	4.546483	-0.008192	1.322786
42.423746	432.959591	4.551488	-0.008360	1.331891
43.044423	441.362513	4.556493	-0.008481	1.340908
43.557209	449.788907	4.561498	-0.008582	1.349870
44.177576	458.193566	4.566502	-0.008704	1.358770
44.668257	466.583467	4.571507	-0.008801	1.367573
45.214988	474.989540	4.576512	-0.008908	1.376346
45.561130	483.386746	4.581517	-0.008978	1.385020
46.338613	491.744127	4.586522	-0.009129	1.393672
47.030808	500.070385	4.591526	-0.009263	1.402225
47.579026	508.408209	4.596531	-0.009371	1.410713
48.312311	516.726023	4.601536	-0.009513	1.419161
48.837922	525.061180	4.606541	-0.009617	1.427542
49.240375	533.423424	4.611546	-0.009698	1.435880
49.713257	541.747085	4.616550	-0.009791	1.444143
50.204099	550.068506	4.621555	-0.009888	1.452360
50.453821	558.420937	4.626560	-0.009941	1.460522
50.891561	566.741904	4.631565	-0.010028	1.468638
51.762158	575.013702	4.636570	-0.010195	1.476731
52.330592	583.280932	4.641574	-0.010307	1.484727
52.620512	591.587603	4.646579	-0.010367	1.492674
53.475253	599.801091	4.651584	-0.010531	1.500579
54.184534	608.040882	4.656589	-0.010669	1.508444
54.759126	616.308157	4.661594	-0.010782	1.516273
55.522822	624.536271	4.666598	-0.010929	1.524053
55.944478	632.819318	4.671603	-0.011014	1.531794
56.489751	641.085416	4.676608	-0.011121	1.539498
56.518498	649.414986	4.681613	-0.011132	1.547145
56.858302	657.698312	4.686618	-0.011201	1.554758
57.529448	665.903509	4.691622	-0.011331	1.562312
57.947893	674.129013	4.696627	-0.011415	1.569810
58.714013	682.351530	4.701632	-0.011563	1.577321
59.015157	690.595131	4.706637	-0.011625	1.584747
59.554442	698.816496	4.711642	-0.011731	1.592153
59.806095	707.068216	4.716646	-0.011783	1.599511
60.243643	715.258818	4.721651	-0.011870	1.606807
60.624958	723.504761	4.726656	-0.011947	1.614111
61.146130	731.691785	4.731661	-0.012050	1.621349
61.642584	739.890005	4.736666	-0.012148	1.628562
62.051295	748.168231	4.741670	-0.012229	1.635800
62.259456	756.368355	4.746675	-0.012274	1.642910
62.663086	764.552586	4.751680	-0.012354	1.650004
63.038919	772.751736	4.756685	-0.012430	1.657075
63.425491	780.929252	4.761690	-0.012508	1.664100
63.814944	789.125668	4.766694	-0.012586	1.671111
64.219792	797.306239	4.771699	-0.012667	1.678081
64.796999	805.449236	4.776704	-0.012780	1.685014
65.302024	813.631310	4.781709	-0.012879	1.691942
65.516594	821.841670	4.786714	-0.012925	1.698826
66.069286	829.994088	4.791718	-0.013033	1.705679
66.123520	838.236722	4.796723	-0.013049	1.712513
66.511779	846.407694	4.801728	-0.013127	1.719305
66.975933	854.539535	4.806733	-0.013219	1.726048
67.446218	862.699476	4.811738	-0.013312	1.732788
67.533208	870.919370	4.816742	-0.013334	1.739501
67.741885	879.069302	4.821747	-0.013378	1.746148
68.393216	887.209736	4.826752	-0.013505	1.752817
68.483323	895.407219	4.831757	-0.013527	1.759436
68.704651	903.561877	4.836762	-0.013574	1.766013
69.527337	911.670918	4.841766	-0.013733	1.772603
69.861739	919.826704	4.846771	-0.013801	1.779146
70.158036	927.997330	4.851776	-0.013861	1.785671
70.587788	936.190307	4.856781	-0.013947	1.792207
71.308325	944.301733	4.861786	-0.014087	1.798690
71.718533	952.421700	4.866790	-0.014169	1.805118
72.091802	960.571354	4.871795	-0.014244	1.811543
72.681959	968.693386	4.876800	-0.014359	1.817949
72.761253	976.866480	4.881805	-0.014379	1.824310
72.994460	985.029168	4.886810	-0.014428	1.830660
73.460268	993.161989	4.891814	-0.014521	1.836993
73.624231	1001.300778	4.896819	-0.014557	1.843273
73.874463	1009.462635	4.901824	-0.014609	1.849559
74.649415	1017.543896	4.906829	-0.014759	1.855823
75.297679	1025.638082	4.911834	-0.014885	1.862061
75.915362	1033.769857	4.916838	-0.015006	1.868303
75.979281	1041.974016	4.921843	-0.015023	1.874515
76.310478	1050.091106	4.926848	-0.015090	1.880672
76.687058	1058.215519	4.931853	-0.015166	1.886819
76.990737	1066.355950	4.936858	-0.015228	1.892950
77.466102	1074.482764	4.941862	-0.015322	1.899070
77.654211	1082.611077	4.946867	-0.015363	1.905139
78.069046	1090.748882	4.951872	-0.015445	1.911221
78.486655	1098.864999	4.956877	-0.015529	1.917268
78.737450	1106.979922	4.961882	-0.015581	1.923276
79.181427	1115.096438	4.966886	-0.015669	1.929289
79.362330	1123.247567	4.971891	-0.015708	1.935278
79.569708	1131.371754	4.976896	-0.015753	1.941233
79.880148	1139.489283	4.981901	-0.015816	1.947175
80.089502	1147.664733	4.986906	-0.015860	1.953131
80.586670	1155.748959	4.991910	-0.015959	1.959033
80.937367	1163.814902	4.996915	-0.016029	1.964889
81.263075	1171.937874	5.001920	-0.016096	1.970765
81.667711	1180.047881	5.006925	-0.016176	1.976623
82.397471	1188.082459	5.011930	-0.016318	1.982444
82.709493	1196.223203	5.016934	-0.016381	1.988280
83.100139	1204.348301	5.021939	-0.016460	1.994095
83.640066	1212.423898	5.026944	-0.016566	1.999874
84.029139	1220.530419	5.031949	-0.016644	2.005642
84.281016	1228.654748	5.036954	-0.016696	2.011392
84.702011	1236.765086	5.041958	-0.016780	2.017133
84.965931	1244.869198	5.046963	-0.016835	2.022837
85.511150	1252.952254	5.051968	-0.016942	2.028539
86.032727	1261.088931	5.056973	-0.017044	2.034260
86.501712	1269.143261	5.061978	-0.017137	2.039903
86.939243	1277.241156	5.066982	-0.017224	2.045556
87.019307	1285.377820	5.071987	-0.017245	2.051184
87.378769	1293.493723	5.076992	-0.017317	2.056811
87.814131	1301.564167	5.081997	-0.017404	2.062399
87.932608	1309.687638	5.087002	-0.017431	2.067976
88.295036	1317.813350	5.092006	-0.017504	2.073564
88.564603	1325.896360	5.097011	-0.017560	2.079099
89.002378	1333.964015	5.102016	-0.017647	2.084624
89.114472	1342.099836	5.107021	-0.017674	2.090150
89.469065	1350.194126	5.112026	-0.017745	2.095656
90.067633	1358.257722	5.117030	-0.017862	2.101151
90.653795	1366.304956	5.122035	-0.017977	2.106620
91.061168	1374.460000	5.127040	-0.018058	2.112129
91.536723	1382.555330	5.132045	-0.018152	2.117590
91.707415	1390.622169	5.137050	-0.018189	2.122988
91.952770	1398.738167	5.142054	-0.018241	2.128413
92.212729	1406.824942	5.147059	-0.018295	2.133806
92.369423	1414.931632	5.152064	-0.018329	2.139189
92.686829	1423.001291	5.157069	-0.018394	2.144549
92.930946	1431.102595	5.162074	-0.018445	2.149909
93.155411	1439.219756	5.167078	-0.018492	2.155264
93.300285	1447.299509	5.172083	-0.018525	2.160575
93.727307	1455.348052	5.177088	-0.018610	2.165878
94.140461	1463.423420	5.182093	-0.018692	2.171184
94.161194	1471.550151	5.187098	-0.018702	2.176474
94.543064	1479.624474	5.192102	-0.018778	2.181751
95.053544	1487.664450	5.197107	-0.018879	2.187004
95.434547	1495.775138	5.202112	-0.018955	2.192279
95.549967	1503.896396	5.207117	-0.018982	2.197523
95.973855	1511.925055	5.212122	-0.019067	2.202723
96.669890	1519.959986	5.217126	-0.019202	2.207940
97.167523	1528.032846	5.222131	-0.019300	2.213150
97.435749	1536.139732	5.227136	-0.019355	2.218350
97.383182	1544.246831	5.232141	-0.019351	2.223508
97.554026	1552.339448	5.237146	-0.019388	2.228665
97.867901	1560.448675	5.242150	-0.019452	2.233834
97.950480	1568.528948	5.247155	-0.019473	2.238951
98.290816	1576.578178	5.252160	-0.019542	2.244061
98.540573	1584.664345	5.257165	-0.019594	2.249173
99.041345	1592.714007	5.262170	-0.019693	2.254273
99.378684	1600.777307	5.267174	-0.019761	2.259356
99.432883	1608.865583	5.272179	-0.019777	2.264419
99.733857	1616.957340	5.277184	-0.019838	2.269493
100.339049	1625.083818	5.282189	-0.019957	2.274604
100.578217	1633.118828	5.287194	-0.020007	2.279615
100.922779	1641.169507	5.292198	-0.020076	2.284634
101.231609	1649.223103	5.297203	-0.020139	2.289640
101.522708	1657.323842	5.302208	-0.020199	2.294663
101.807198	1665.381520	5.307213	-0.020257	2.299648
101.659214	1673.485724	5.312218	-0.020235	2.304614
101.952039	1681.568574	5.317222	-0.020295	2.309594
102.189282	1689.644755	5.322227	-0.020345	2.314554
102.487129	1697.677412	5.327232	-0.020406	2.319482
102.924995	1705.717240	5.332237	-0.020493	2.324415
103.359274	1713.748722	5.337242	-0.020579	2.329332
103.592952	1721.870387	5.342246	-0.020628	2.334277
103.851044	1729.940286	5.347251	-0.020682	2.339182
104.016940	1738.018863	5.352256	-0.020718	2.344075
104.366087	1746.076909	5.357261	-0.020789	2.348959
104.556057	1754.185984	5.362266	-0.020830	2.353852
104.832332	1762.232975	5.367270	-0.020887	2.358704
104.931370	1770.300553	5.372275	-0.020911	2.363544
105.529746	1778.331076	5.377280	-0.021028	2.368392
106.017527	1786.405919	5.382285	-0.021124	2.373247
106.080219	1794.475975	5.387290	-0.021141	2.378056
106.127256	1802.580040	5.392294	-0.021155	2.382874
106.310026	1810.635455	5.397299	-0.021195	2.387664
106.624149	1818.707308	5.402304	-0.021259	2.392464
106.767686	1826.793232	5.407309	-0.021291	2.397250
107.039378	1834.821056	5.412314	-0.021347	2.402002
107.610271	1842.863127	5.417318	-0.021459	2.406776
107.995488	1850.926270	5.422323	-0.021536	2.411539
107.977177	1859.036511	5.427328	-0.021538	2.416288
108.181699	1867.097357	5.432333	-0.021582	2.421017
108.368036	1875.148127	5.437338	-0.021622	2.425729
108.850978	1883.221097	5.442342	-0.021718	2.430467
109.097443	1891.341893	5.447347	-0.021769	2.435206
109.349255	1899.364839	5.452352	-0.021821	2.439879
109.682066	1907.389444	5.457357	-0.021889	2.444550
109.870304	1915.432122	5.462362	-0.021929	2.449212
110.094555	1923.522376	5.467366	-0.021977	2.453895
110.110503	1931.578981	5.472371	-0.021985	2.458534
110.489189	1939.599572	5.477376	-0.022061	2.463171
110.855518	1947.662210	5.482381	-0.022135	2.467822
111.043717	1955.727226	5.487386	-0.022175	2.472452
111.352807	1963.789016	5.492390	-0.022238	2.477081
111.487996	1971.842122	5.497395	-0.022269	2.481683
112.018804	1979.862210	5.502400	-0.022373	2.486288
112.369306	1987.937109	5.507405	-0.022444	2.490901
112.492490	1996.018331	5.512410	-0.022473	2.495493
112.595736	2004.114619	5.517414	-0.022497	2.500083
112.962433	2012.113605	5.522419	-0.022571	2.504629
113.224597	2020.191532	5.527424	-0.022625	2.509204
113.515292	2028.306520	5.532429	-0.022685	2.513793
113.815324	2036.321323	5.537434	-0.022746	2.518318
114.150935	2044.361776	5.542438	-0.022814	2.522852
114.382971	2052.406176	5.547443	-0.022863	2.527373
114.813241	2060.441743	5.552448	-0.022949	2.531894
115.003384	2068.542493	5.557453	-0.022990	2.536427
115.052561	2076.589134	5.562458	-0.023004	2.540911
115.384265	2084.641899	5.567462	-0.023071	2.545411
115.609989	2092.689371	5.572467	-0.023119	2.549893
115.903931	2100.737417	5.577472	-0.023179	2.554371
116.269444	2108.786473	5.582477	-0.023253	2.558848
116.484982	2116.809953	5.587482	-0.023298	2.563292
116.643406	2124.908869	5.592486	-0.023333	2.567765
116.768290	2132.987047	5.597491	-0.023362	2.572217
117.236302	2141.014198	5.602496	-0.023455	2.576657
117.569041	2149.059384	5.607501	-0.023522	2.581090
117.624506	2157.105733	5.612506	-0.023538	2.585497
118.006062	2165.185621	5.617510	-0.023615	2.589937
118.104693	2173.436780	5.622515	-0.023639	2.594443
118.593305	2181.378982	5.627520	-0.023735	2.598800
119.092528	2189.362526	5.632525	-0.023833	2.603173
119.515961	2197.367800	5.637530	-0.023918	2.607545
119.659473	2205.468307	5.642534	-0.023950	2.611942
120.123482	2213.482675	5.647539	-0.024042	2.616307
120.309628	2221.535314	5.652544	-0.024082	2.620666
120.634349	2229.566069	5.657549	-0.024148	2.625016
121.121433	2237.574605	5.662554	-0.024244	2.629357
121.534183	2245.660530	5.667558	-0.024326	2.633727
121.589479	2253.717635	5.672563	-0.024342	2.638052
121.961038	2261.723431	5.677568	-0.024417	2.642362
122.472227	2269.772448	5.682573	-0.024518	2.646698
122.568695	2277.859167	5.687578	-0.024541	2.651019
122.709607	2285.946377	5.692582	-0.024573	2.655336
123.074608	2293.939562	5.697587	-0.024646	2.659611
123.422808	2301.976125	5.702592	-0.024717	2.663901
123.815914	2310.030998	5.707597	-0.024795	2.668197
123.807032	2318.156828	5.712602	-0.024799	2.672497
124.383504	2326.176792	5.717606	-0.024912	2.676772
124.845418	2334.183535	5.722611	-0.025003	2.681026
124.832010	2342.244185	5.727616	-0.025006	2.685271
125.115000	2350.277621	5.732621	-0.025065	2.689513
125.414325	2358.340989	5.737626	-0.025126	2.693766
125.743065	2366.391092	5.742630	-0.025193	2.698007
125.723391	2374.452971	5.747635	-0.025194	2.702226
125.770091	2382.511108	5.752640	-0.025209	2.706440
126.075760	2390.562183	5.757645	-0.025271	2.710660
126.358310	2398.593970	5.762650	-0.025329	2.714862
126.645403	2406.637830	5.767654	-0.025388	2.719064
126.923218	2414.645479	5.772659	-0.025445	2.723240
127.094994	2422.705930	5.777664	-0.025483	2.727430
127.602312	2430.767967	5.782669	-0.025583	2.731635
127.887289	2438.806256	5.787674	-0.025641	2.735808
128.188261	2446.848436	5.792678	-0.025703	2.739978
128.219135	2454.891949	5.797683	-0.025714	2.744125
128.448949	2462.923558	5.802688	-0.025762	2.748272
128.925637	2471.031982	5.807693	-0.025857	2.752467
129.007171	2479.103947	5.812698	-0.025877	2.756613
129.295538	2487.139419	5.817702	-0.025936	2.760746
129.574202	2495.132658	5.822707	-0.025994	2.764851
129.936700	2503.159935	5.827712	-0.026067	2.768973
130.262649	2511.217751	5.832717	-0.026133	2.773101
130.297867	2519.266478	5.837722	-0.026145	2.777202
130.606286	2527.302668	5.842726	-0.026208	2.781306
130.667349	2535.343991	5.847731	-0.026225	2.785392
130.906433	2543.388201	5.852736	-0.026275	2.789484
131.602853	2551.434551	5.857741	-0.026410	2.793598
131.676234	2559.474405	5.862746	-0.026429	2.797666
132.099610	2567.503523	5.867750	-0.026513	2.801743
132.239374	2575.540719	5.872755	-0.026545	2.805802
132.459880	2583.600829	5.877760	-0.026591	2.809870
132.897609	2591.649647	5.882765	-0.026678	2.813940
133.067457	2599.691925	5.887770	-0.026716	2.817985
133.439671	2607.723923	5.892774	-0.026790	2.822031
133.397950	2615.808761	5.897779	-0.026788	2.826074
133.396860	2623.845493	5.902784	-0.026793	2.830089
133.867367	2631.915665	5.907789	-0.026886	2.834142
134.055501	2639.909381	5.912794	-0.026927	2.838135
134.485141	2647.919060	5.917798	-0.027012	2.842144
134.813656	2655.936039	5.922803	-0.027079	2.846145
134.916221	2663.987548	5.927808	-0.027104	2.850145
135.209252	2672.045305	5.932813	-0.027164	2.854153
135.610182	2680.068913	5.937818	-0.027244	2.858145
135.865972	2688.126635	5.942822	-0.027297	2.862139
135.923124	2696.177560	5.947827	-0.027313	2.866114
136.078961	2704.218478	5.952832	-0.027348	2.870084
136.415014	2712.297429	5.957837	-0.027416	2.874076
136.438517	2720.310192	5.962842	-0.027425	2.878014
136.860800	2728.333371	5.967846	-0.027510	2.881973
137.039723	2736.380274	5.972851	-0.027548	2.885925
137.169620	2744.395871	5.977856	-0.027578	2.889853
137.461348	2752.496567	5.982861	-0.027638	2.893826
137.554406	2760.513402	5.987866	-0.027661	2.897743
137.877404	2768.549678	5.992870	-0.027726	2.901675
137.854755	2776.612109	5.997875	-0.027728	2.905597
138.035458	2784.629568	6.002880	-0.027767	2.909502
138.342578	2792.778552	6.007885	-0.027829	2.913473
138.795628	2800.739046	6.012890	-0.027919	2.917354
139.077956	2808.763334	6.017894	-0.027977	2.921253
139.363542	2816.762589	6.022899	-0.028036	2.925134
139.448225	2824.791998	6.027904	-0.028057	2.929013
139.606254	2832.876607	6.032909	-0.028092	2.932918
139.768128	2840.884043	6.037914	-0.028128	2.936781
139.916664	2848.930213	6.042918	-0.028161	2.940657
140.184448	2856.933146	6.047923	-0.028216	2.944513
140.265025	2865.005445	6.052928	-0.028237	2.948387
140.338615	2873.086559	6.057933	-0.028256	2.952260
140.506853	2881.091025	6.062938	-0.028293	2.956097
140.650902	2889.131487	6.067942	-0.028325	2.959944
140.827101	2897.152182	6.072947	-0.028363	2.963778
140.927849	2905.187530	6.077952	-0.028388	2.967611
140.979283	2913.258969	6.082957	-0.028403	2.971453
141.190725	2921.277745	6.087962	-0.028447	2.975274
141.671491	2929.294652	6.092966	-0.028542	2.979102
141.713797	2937.335898	6.097971	-0.028556	2.982914
141.910118	2945.363157	6.102976	-0.028598	2.986723
142.148720	2953.421401	6.107981	-0.028648	2.990544
142.793010	2961.440467	6.112986	-0.028773	2.994361
142.836861	2969.485263	6.117990	-0.028787	2.998156
143.206753	2977.484620	6.122995	-0.028861	3.001941
143.486841	2985.505068	6.128000	-0.028919	3.005726
143.638822	2993.569880	6.133005	-0.028953	3.009522
143.729083	3001.644781	6.138010	-0.028975	3.013314
143.985951	3009.667765	6.143014	-0.029028	3.017085
144.127361	3017.706332	6.148019	-0.029060	3.020853
144.259154	3025.726604	6.153024	-0.029090	3.024607
144.523291	3033.787302	6.158029	-0.029145	3.028382
144.695595	3041.820172	6.163034	-0.029182	3.032134
144.956295	3049.878740	6.168038	-0.029236	3.035898
145.141490	3057.862560	6.173043	-0.029276	3.039620
145.483381	3065.879072	6.178048	-0.029345	3.043359
145.706916	3073.930646	6.183053	-0.029393	3.047104
145.680427	3081.982278	6.188058	-0.029393	3.050833
146.200258	3090.002408	6.193062	-0.029495	3.054568
146.598164	3098.032982	6.198067	-0.029575	3.058298
146.684151	3106.071695	6.203072	-0.029596	3.062012
146.875038	3114.121012	6.208077	-0.029637	3.065732
147.107904	3122.126394	6.213082	-0.029686	3.069428
147.149410	3130.294882	6.218086	-0.029700	3.073187
147.045805	3138.335799	6.223091	-0.029686	3.076875
147.288328	3146.317819	6.228096	-0.029736	3.080548
147.626033	3154.284172	6.233101	-0.029805	3.084214
147.418249	3162.336502	6.238106	-0.029772	3.087889
147.776144	3170.372675	6.243110	-0.029844	3.091579
148.116392	3178.409469	6.248115	-0.029912	3.095264
148.357463	3186.402283	6.253120	-0.029963	3.098920
148.607283	3194.455227	6.258125	-0.030015	3.102599
148.641369	3202.498269	6.263130	-0.030027	3.106260
148.979433	3210.526629	6.268134	-0.030095	3.109923
149.258760	3218.566364	6.273139	-0.030153	3.113585
149.499996	3226.564376	6.278144	-0.030203	3.117221
149.718536	3234.639655	6.283149	-0.030249	3.120887
149.785170	3242.623567	6.288154	-0.030267	3.124501
150.139149	3250.659554	6.293158	-0.030338	3.128147
150.347219	3258.736132	6.298163	-0.030383	3.131800
150.651892	3266.768367	6.303168	-0.030445	3.135434
150.802555	3274.809273	6.308173	-0.030478	3.139060
150.777674	3282.817046	6.313178	-0.030479	3.142659
151.216480	3290.835158	6.318182	-0.030566	3.146280
151.252738	3298.893747	6.323187	-0.030579	3.149896
151.497114	3306.960134	6.328192	-0.030630	3.153521
151.848903	3314.955671	6.333197	-0.030701	3.157115
151.921148	3322.975799	6.338202	-0.030720	3.160703
151.992297	3330.983505	6.343206	-0.030738	3.164282
152.274422	3339.013508	6.348211	-0.030796	3.167876
152.536110	3347.058961	6.353216	-0.030850	3.171471
152.753576	3355.119351	6.358221	-0.030896	3.175068
152.814254	3363.135918	6.363226	-0.030913	3.178634
153.116731	3371.170663	6.368230	-0.030975	3.182214
153.368904	3379.187742	6.373235	-0.031027	3.185780
153.493904	3387.228923	6.378240	-0.031056	3.189348
153.727132	3395.295671	6.383245	-0.031105	3.192927
153.752658	3403.317882	6.388250	-0.031115	3.196474
154.182191	3411.316980	6.393254	-0.031201	3.200024
154.544245	3419.325208	6.398259	-0.031274	3.203571
154.526707	3427.401841	6.403264	-0.031276	3.207128
154.657608	3435.459925	6.408269	-0.031306	3.210679
155.042829	3443.439772	6.413274	-0.031383	3.214203
155.272950	3451.507200	6.418278	-0.031431	3.217754
155.304389	3459.535368	6.423283	-0.031443	3.221276
155.347708	3467.526311	6.428288	-0.031456	3.224779
155.834029	3475.569487	6.433293	-0.031552	3.228319
155.961857	3483.637328	6.438298	-0.031582	3.231851
156.135203	3491.735580	6.443302	-0.031619	3.235394
156.666903	3499.684171	6.448307	-0.031724	3.238882
156.702865	3507.707646	6.453312	-0.031736	3.242380
156.921535	3515.730796	6.458317	-0.031782	3.245880
157.057580	3523.722931	6.463322	-0.031813	3.249360
157.385598	3531.765717	6.468326	-0.031880	3.252866
157.622991	3539.802641	6.473331	-0.031929	3.256362
157.762362	3547.802536	6.478336	-0.031961	3.259835
157.893286	3555.842839	6.483341	-0.031990	3.263320
158.017229	3563.901839	6.488346	-0.032019	3.266810
158.025052	3571.948294	6.493350	-0.032026	3.270286
158.501363	3579.988206	6.498355	-0.032120	3.273774
158.648104	3587.989310	6.503360	-0.032153	3.277229
158.820704	3596.008925	6.508365	-0.032191	3.280688
158.942251	3604.007579	6.513370	-0.032219	3.284134
159.288887	3612.060551	6.518374	-0.032289	3.287607
159.486345	3620.103622	6.523379	-0.032331	3.291067
159.383946	3628.147950	6.528384	-0.032317	3.294512
159.771708	3636.172773	6.533389	-0.032395	3.297964
159.850794	3644.206790	6.538394	-0.032415	3.301404
159.917986	3652.203521	6.543398	-0.032433	3.304825
160.316421	3660.244195	6.548403	-0.032513	3.308273
160.417317	3668.300852	6.553408	-0.032537	3.311713
160.592081	3676.371857	6.558413	-0.032575	3.315159
160.808863	3684.324340	6.563418	-0.032621	3.318552
160.911739	3692.361979	6.568422	-0.032646	3.321973
161.075594	3700.376117	6.573427	-0.032682	3.325383
161.207092	3708.394785	6.578432	-0.032712	3.328791
161.641924	3716.462943	6.583437	-0.032798	3.332227
161.845919	3724.457299	6.588442	-0.032841	3.335619
161.967145	3732.480417	6.593446	-0.032870	3.339018
162.170407	3740.508325	6.598451	-0.032913	3.342418
162.559725	3748.518724	6.603456	-0.032991	3.345813
162.613740	3756.608747	6.608461	-0.033006	3.349227
162.768859	3764.618975	6.613466	-0.033041	3.352607
163.288771	3772.657096	6.618470	-0.033143	3.356009
163.455991	3780.656731	6.623475	-0.033180	3.359378
163.404146	3788.677356	6.628480	-0.033175	3.362745
163.627193	3796.733806	6.633485	-0.033222	3.366133
163.770310	3804.759865	6.638490	-0.033255	3.369503
163.955294	3812.807617	6.643494	-0.033295	3.372879
164.149147	3820.832905	6.648499	-0.033336	3.376243
164.370724	3828.834043	6.653504	-0.033383	3.379594
164.494073	3836.901691	6.658509	-0.033411	3.382967
164.626738	3844.916002	6.663514	-0.033441	3.386314
164.916817	3852.922783	6.668518	-0.033501	3.389660
165.210318	3861.033392	6.673523	-0.033561	3.393046
165.393265	3869.045847	6.678528	-0.033601	3.396384
165.724269	3877.029061	6.683533	-0.033668	3.399712
165.949150	3885.017839	6.688538	-0.033715	3.403035
166.054355	3893.044861	6.693542	-0.033740	3.406367
166.307690	3901.051638	6.698547	-0.033793	3.409691
166.449344	3909.106578	6.703552	-0.033825	3.413029
166.615992	3917.146249	6.708557	-0.033861	3.416358
166.963868	3925.114584	6.713562	-0.033931	3.419661
167.180953	3933.171226	6.718566	-0.033977	3.422992
167.362019	3941.212263	6.723571	-0.034016	3.426312
167.171571	3949.266631	6.728576	-0.033987	3.429622
167.428125	3957.319457	6.733581	-0.034040	3.432943
167.641440	3965.334335	6.738586	-0.034085	3.436244
167.831635	3973.319347	6.743590	-0.034126	3.439529
167.698499	3981.361965	6.748595	-0.034107	3.442823
168.044908	3989.382511	6.753600	-0.034177	3.446121
168.421232	3997.403913	6.758605	-0.034252	3.449417
168.483035	4005.454723	6.763610	-0.034269	3.452712
168.863332	4013.493747	6.768614	-0.034345	3.456009
169.081677	4021.490121	6.773619	-0.034391	3.459280
169.163201	4029.508959	6.778624	-0.034412	3.462553
169.405558	4037.560915	6.783629	-0.034463	3.465842
169.636444	4045.563230	6.788634	-0.034511	3.469106
169.877451	4053.656888	6.793638	-0.034562	3.472405
170.061413	4061.663704	6.798643	-0.034601	3.475664
170.232890	4069.629862	6.803648	-0.034639	3.478903
170.413016	4077.684499	6.808653	-0.034678	3.482175
170.514153	4085.657413	6.813658	-0.034702	3.485408
170.883170	4093.700871	6.818662	-0.034776	3.488675
171.133305	4101.735096	6.823667	-0.034828	3.491932
171.190067	4109.788958	6.828672	-0.034844	3.495187
171.464915	4117.817115	6.833677	-0.034901	3.498436
171.509008	4125.818906	6.838682	-0.034915	3.501663
171.884442	4133.817922	6.843686	-0.034990	3.504898
171.922665	4141.861455	6.848691	-0.035003	3.508136
172.179752	4149.889345	6.853696	-0.035056	3.511372
172.636908	4157.915589	6.858701	-0.035147	3.514610
172.751600	4165.937610	6.863706	-0.035173	3.517834
172.892504	4173.986073	6.868710	-0.035205	3.521065
173.044265	4181.960087	6.873715	-0.035239	3.524264
173.481329	4189.978218	6.878720	-0.035326	3.527487
173.551185	4198.052101	6.883725	-0.035344	3.530717
173.505220	4206.103105	6.888730	-0.035341	3.533933
173.899254	4214.106255	6.893734	-0.035420	3.537139
174.185986	4222.129644	6.898739	-0.035479	3.540347
174.241349	4230.137868	6.903744	-0.035495	3.543539
174.420007	4238.211580	6.908749	-0.035533	3.546758
174.472417	4246.240116	6.913754	-0.035549	3.549953
174.857337	4254.332072	6.918758	-0.035626	3.553179
175.287101	4262.381022	6.923763	-0.035711	3.556387
175.319434	4270.285022	6.928768	-0.035723	3.559523
175.574707	4278.333214	6.933773	-0.035776	3.562720
175.642535	4286.316603	6.938778	-0.035794	3.565882
175.748747	4294.347722	6.943782	-0.035819	3.569062
176.104309	4302.384342	6.948787	-0.035891	3.572248
176.276175	4310.392718	6.953792	-0.035928	3.575415
176.455142	4318.404593	6.958797	-0.035967	3.578581
176.559427	4326.447321	6.963802	-0.035992	3.581754
176.658437	4334.477789	6.968806	-0.036016	3.584919
176.700335	4342.526691	6.973811	-0.036029	3.588087
176.739652	4350.538422	6.978816	-0.036042	3.591237
177.156676	4358.567364	6.983821	-0.036125	3.594402
177.181013	4366.562560	6.988826	-0.036135	3.597540
177.298698	4374.586742	6.993830	-0.036162	3.600689
177.534983	4382.558497	6.998835	-0.036212	3.603819
177.769671	4390.619611	7.003840	-0.036261	3.606980
178.096861	4398.637399	7.008845	-0.036327	3.610124
178.037119	4406.660993	7.013850	-0.036322	3.613257
178.362767	4414.718686	7.018854	-0.036388	3.616411
178.499952	4422.691945	7.023859	-0.036419	3.619524
178.903861	4430.732733	7.028864	-0.036500	3.622669
179.162014	4438.807770	7.033869	-0.036553	3.625819
179.006672	4446.802444	7.038874	-0.036530	3.628925
179.591403	4454.850330	7.043878	-0.036644	3.632068
179.635129	4462.931025	7.048883	-0.036658	3.635207
179.498514	4470.908064	7.053888	-0.036638	3.638298
179.877736	4478.932701	7.058893	-0.036714	3.641419
180.184754	4486.897604	7.063898	-0.036776	3.644512
180.316746	4494.943608	7.068902	-0.036806	3.647629
180.709964	4502.981068	7.073907	-0.036885	3.650747
180.672765	4511.008933	7.078912	-0.036884	3.653847
181.133991	4519.054934	7.083917	-0.036975	3.656965
181.187102	4527.032906	7.088922	-0.036990	3.660043
181.503371	4535.060577	7.093926	-0.037055	3.663144
181.660615	4543.114877	7.098931	-0.037090	3.666249
181.882016	4551.091370	7.103936	-0.037136	3.669323
181.942207	4559.187079	7.108941	-0.037153	3.672436
182.158378	4567.164553	7.113946	-0.037199	3.675505
182.348300	4575.179043	7.118950	-0.037240	3.678585
182.835518	4583.209048	7.123955	-0.037336	3.681675
182.857063	4591.189714	7.128960	-0.037345	3.684733
182.851392	4599.274313	7.133965	-0.037350	3.687827
183.011379	4607.289421	7.138970	-0.037385	3.690896
183.387621	4615.308481	7.143974	-0.037460	3.693969
183.408134	4623.359389	7.148979	-0.037470	3.697043
183.491278	4631.338399	7.153984	-0.037491	3.700088
183.806953	4639.371132	7.158989	-0.037555	3.703158
184.087475	4647.368674	7.163994	-0.037613	3.706210
184.400649	4655.374927	7.168998	-0.037676	3.709264
184.412413	4663.511763	7.174003	-0.037684	3.712357
184.802677	4671.543829	7.179008	-0.037762	3.715418
185.092966	4679.516707	7.184013	-0.037822	3.718451
185.077282	4687.550435	7.189018	-0.037824	3.721497
185.273851	4695.488158	7.194022	-0.037866	3.724510
185.327655	4703.533894	7.199027	-0.037882	3.727557
185.393697	4711.533452	7.204032	-0.037900	3.730585
185.799266	4719.601503	7.209037	-0.037981	3.733644
185.703551	4727.633574	7.214042	-0.037968	3.736675
185.998481	4735.590438	7.219046	-0.038029	3.739685
186.294174	4743.647404	7.224051	-0.038089	3.742730
186.250395	4751.665151	7.229056	-0.038087	3.745749
186.345127	4759.723864	7.234061	-0.038110	3.748785
186.400008	4767.750117	7.239066	-0.038125	3.751805
186.741623	4775.774244	7.244070	-0.038194	3.754829
187.166688	4783.777387	7.249075	-0.038279	3.757844
187.168053	4791.771620	7.254080	-0.038285	3.760844
187.477722	4799.802471	7.259085	-0.038348	3.763862
187.765178	4807.813757	7.264090	-0.038407	3.766870
187.875076	4815.858263	7.269094	-0.038433	3.769883
188.070454	4823.915757	7.274099	-0.038475	3.772901
188.271641	4831.937656	7.279104	-0.038518	3.775904
188.693691	4839.945168	7.284109	-0.038602	3.778903
188.695092	4847.955262	7.289114	-0.038607	3.781892
188.802175	4855.969547	7.294118	-0.038633	3.784882
189.106416	4864.001907	7.299123	-0.038695	3.787881
189.123540	4872.036915	7.304128	-0.038704	3.790872
189.300097	4880.130951	7.309133	-0.038742	3.793887
189.525065	4888.102579	7.314138	-0.038789	3.796854
189.704916	4896.071437	7.319142	-0.038828	3.799817
190.090957	4904.074871	7.324147	-0.038906	3.802795
190.295445	4912.108039	7.329152	-0.038949	3.805778
190.449447	4920.126951	7.334157	-0.038983	3.808752
190.310266	4928.204723	7.339162	-0.038963	3.811739
190.660185	4936.169184	7.344166	-0.039034	3.814693
190.915238	4944.220676	7.349171	-0.039087	3.817674
191.057375	4952.197139	7.354176	-0.039118	3.820623
191.319262	4960.245738	7.359181	-0.039173	3.823598
191.676588	4968.253755	7.364186	-0.039245	3.826558
191.673437	4976.295499	7.369190	-0.039250	3.829521
191.671001	4984.361251	7.374195	-0.039255	3.832491
191.934983	4992.350238	7.379200	-0.039309	3.835435
192.184953	5000.364120	7.384205	-0.039361	3.838386
192.229086	5008.384822	7.389210	-0.039375	3.841333
192.364516	5016.361483	7.394214	-0.039406	3.844263
192.704501	5024.406099	7.399219	-0.039474	3.847220
192.670829	5032.402880	7.404224	-0.039474	3.850150
192.707737	5040.504180	7.409229	-0.039486	3.853117
192.945994	5048.537439	7.414234	-0.039536	3.856061
192.965210	5056.532645	7.419238	-0.039545	3.858985
193.302095	5064.560929	7.424243	-0.039613	3.861924
193.475067	5072.526601	7.429248	-0.039651	3.864835
193.699189	5080.597461	7.434253	-0.039698	3.867784
193.611740	5088.614404	7.439258	-0.039687	3.870704
194.070619	5096.885621	7.444262	-0.039778	3.873726
194.375359	5104.857717	7.449267	-0.039840	3.876633
194.518635	5112.703766	7.454272	-0.039872	3.879489
194.572830	5120.734915	7.459277	-0.039888	3.882408
195.095204	5128.717038	7.464282	-0.039991	3.885317
195.277973	5136.727743	7.469286	-0.040030	3.888227
195.178697	5144.759485	7.474291	-0.040017	3.891137
195.444588	5152.794301	7.479296	-0.040072	3.894053
195.999089	5160.800234	7.484301	-0.040181	3.896962
195.972734	5168.776360	7.489306	-0.040181	3.899846
196.163998	5176.815281	7.494310	-0.040223	3.902756
196.480538	5184.870203	7.499315	-0.040287	3.905671
196.435539	5192.854839	7.504320	-0.040284	3.908552
196.592397	5200.937116	7.509325	-0.040319	3.911470
196.865226	5208.932009	7.514330	-0.040375	3.914356
197.106592	5216.938007	7.519334	-0.040425	3.917244
197.189726	5224.949423	7.524339	-0.040446	3.920128
197.275831	5232.943181	7.529344	-0.040468	3.923004
197.633698	5240.987316	7.534349	-0.040540	3.925901
197.665972	5248.979180	7.539354	-0.040551	3.928771
197.876547	5257.024526	7.544358	-0.040596	3.931661
198.112799	5265.043244	7.549363	-0.040646	3.934540
198.101875	5273.056737	7.554368	-0.040649	3.937411
198.186787	5281.087894	7.559373	-0.040670	3.940288
198.268897	5289.092800	7.564378	-0.040691	3.943153
198.483684	5297.110134	7.569382	-0.040737	3.946023
198.578859	5305.147147	7.574387	-0.040760	3.948895
198.620516	5313.190053	7.579392	-0.040773	3.951767
199.120776	5321.225249	7.584397	-0.040872	3.954641
199.136124	5329.225199	7.589402	-0.040880	3.957493
199.301438	5337.192995	7.594406	-0.040916	3.960334
199.766462	5345.220608	7.599411	-0.041008	3.963199
199.737429	5353.235770	7.604416	-0.041008	3.966049
199.912320	5361.259259	7.609421	-0.041046	3.968903
200.064396	5369.326627	7.614426	-0.041080	3.971771
200.243129	5377.352872	7.619430	-0.041119	3.974622
200.350034	5385.391875	7.624435	-0.041144	3.977475
200.273892	5393.378317	7.629440	-0.041136	3.980304
200.827729	5401.383285	7.634445	-0.041244	3.983148
200.911391	5409.386107	7.639450	-0.041265	3.985981
200.764599	5417.423020	7.644454	-0.041243	3.988820
201.066320	5425.497921	7.649459	-0.041305	3.991678
201.570936	5433.501307	7.654464	-0.041404	3.994513
201.832260	5441.538558	7.659469	-0.041459	3.997353
201.881500	5449.525767	7.664474	-0.041473	4.000170
201.998544	5457.542149	7.669478	-0.041500	4.002996
202.171447	5465.572371	7.674483	-0.041538	4.005826
202.226999	5473.560377	7.679488	-0.041554	4.008637
202.315146	5481.644054	7.684493	-0.041576	4.011481
202.376994	5489.652016	7.689498	-0.041593	4.014295
202.524941	5497.671591	7.694502	-0.041626	4.017113
202.855312	5505.652299	7.699507	-0.041693	4.019918
202.949567	5513.667835	7.704512	-0.041716	4.022730
203.204421	5521.712292	7.709517	-0.041769	4.025552
203.475945	5529.717179	7.714522	-0.041825	4.028359
203.650163	5537.753424	7.719526	-0.041863	4.031173
203.765198	5545.887259	7.724531	-0.041890	4.034019
203.802782	5553.873787	7.729536	-0.041902	4.036809
204.105106	5561.799052	7.734541	-0.041964	4.039581
204.046382	5569.808861	7.739546	-0.041958	4.042374
204.203286	5577.806970	7.744550	-0.041993	4.045165
204.483423	5585.858353	7.749555	-0.042051	4.047974
204.601947	5593.848700	7.754560	-0.042078	4.050758
204.827005	5601.902973	7.759565	-0.042126	4.053563
205.021225	5609.928282	7.764570	-0.042167	4.056356
205.220188	5617.870920	7.769574	-0.042210	4.059119
205.464432	5625.915238	7.774579	-0.042261	4.061915
205.392414	5633.890899	7.779584	-0.042253	4.064681
205.509906	5641.951590	7.784589	-0.042280	4.067478
205.672493	5649.979992	7.789594	-0.042316	4.070261
205.837903	5658.032795	7.794598	-0.042352	4.073052
206.067948	5666.069633	7.799603	-0.042401	4.075836
206.115185	5674.022761	7.804608	-0.042415	4.078586
206.340856	5682.081716	7.809613	-0.042462	4.081374
206.598250	5690.051857	7.814618	-0.042516	4.084129
206.626401	5698.076393	7.819622	-0.042526	4.086899
206.912776	5706.104374	7.824627	-0.042585	4.089671
207.103079	5714.133536	7.829632	-0.042626	4.092440
207.342857	5722.188970	7.834637	-0.042676	4.095217
207.625298	5730.158472	7.839642	-0.042734	4.097963
207.676027	5738.176900	7.844646	-0.042749	4.100721
207.966773	5746.198808	7.849651	-0.042809	4.103481
208.077522	5754.224939	7.854656	-0.042835	4.106239
208.153101	5762.246936	7.859661	-0.042854	4.108993
208.106619	5770.314485	7.864666	-0.042851	4.111759
208.395401	5778.343859	7.869670	-0.042910	4.114515
208.705667	5786.372468	7.874675	-0.042974	4.117268
208.736220	5794.339439	7.879680	-0.042985	4.119995
208.901912	5802.364229	7.884685	-0.043021	4.122742
209.142498	5810.353312	7.889690	-0.043071	4.125476
209.134784	5818.392560	7.894694	-0.043075	4.128221
209.275481	5826.425351	7.899699	-0.043107	4.130965
209.580486	5834.430123	7.904704	-0.043169	4.133699
209.889536	5842.514395	7.909709	-0.043232	4.136459
209.989143	5850.467776	7.914714	-0.043256	4.139169
210.270108	5858.492424	7.919718	-0.043314	4.141904
210.495916	5866.489572	7.924723	-0.043362	4.144628
210.585288	5874.552932	7.929728	-0.043384	4.147370
210.577826	5882.572675	7.934733	-0.043388	4.150095
210.946813	5890.598355	7.939738	-0.043462	4.152824
211.025120	5898.611948	7.944742	-0.043482	4.155544
211.525288	5906.606143	7.949747	-0.043581	4.158260
211.487304	5914.618713	7.954752	-0.043579	4.160975
211.499104	5922.636654	7.959757	-0.043587	4.163690
211.602065	5930.687204	7.964762	-0.043612	4.166416
211.830829	5938.663107	7.969766	-0.043660	4.169116
212.414542	5946.687826	7.974771	-0.043774	4.171834
212.448778	5954.725249	7.979776	-0.043786	4.174549
212.564466	5962.769853	7.984781	-0.043813	4.177266
212.751859	5970.747018	7.989786	-0.043853	4.179958
212.629551	5978.771982	7.994790	-0.043836	4.182662
213.100529	5986.790198	7.999795	-0.043929	4.185368
213.256717	5994.790594	8.004800	-0.043963	4.188063
213.396146	6002.856166	8.009805	-0.043995	4.190778
213.648048	6010.942947	8.014810	-0.044047	4.193499
213.821180	6018.967880	8.019814	-0.044085	4.196197
214.203972	6026.889120	8.024819	-0.044162	4.198861
214.253193	6034.889313	8.029824	-0.044176	4.201546
214.396226	6042.868442	8.034829	-0.044208	4.204223
214.588719	6050.922949	8.039834	-0.044250	4.206924
214.636516	6058.910708	8.044838	-0.044264	4.209600
214.727371	6066.969444	8.049843	-0.044286	4.212298
214.935637	6074.941117	8.054848	-0.044331	4.214966
215.225063	6082.988359	8.059853	-0.044390	4.217659
215.240800	6090.996732	8.064858	-0.044398	4.220334
215.390004	6099.001541	8.069862	-0.044432	4.223008
215.700756	6107.026363	8.074867	-0.044495	4.225688
215.845767	6115.031319	8.079872	-0.044527	4.228358
216.036279	6123.053195	8.084877	-0.044568	4.231033
216.239096	6131.084564	8.089882	-0.044612	4.233709
216.510585	6139.144464	8.094886	-0.044668	4.236394
216.670217	6147.141429	8.099891	-0.044703	4.239055
216.436768	6155.168776	8.104896	-0.044665	4.241720
216.905071	6163.105081	8.109901	-0.044758	4.244361
217.008038	6171.183804	8.114906	-0.044782	4.247043
217.191960	6179.157157	8.119910	-0.044822	4.249689
217.376794	6187.296634	8.124915	-0.044862	4.252389
217.582674	6195.223970	8.129920	-0.044906	4.255017
217.742191	6203.283963	8.134925	-0.044941	4.257687
218.050227	6211.268610	8.139930	-0.045004	4.260332
218.121809	6219.294936	8.144934	-0.045022	4.262987
218.075269	6227.326623	8.149939	-0.045019	4.265640
218.244527	6235.395403	8.154944	-0.045056	4.268307
218.469833	6243.378884	8.159949	-0.045104	4.270943
218.619038	6251.458388	8.164954	-0.045137	4.273610
218.821589	6259.445933	8.169958	-0.045180	4.276244
219.113691	6267.424812	8.174963	-0.045240	4.278875
219.169421	6275.444173	8.179968	-0.045256	4.281516
219.126497	6283.415964	8.184973	-0.045253	4.284138
219.306066	6291.495306	8.189978	-0.045292	4.286796
219.501493	6299.490014	8.194982	-0.045334	4.289425
219.704733	6307.542773	8.199987	-0.045377	4.292071
219.696495	6315.537278	8.204992	-0.045381	4.294695
219.808497	6323.594681	8.209997	-0.045408	4.297339
220.133183	6331.560494	8.215002	-0.045474	4.299952
220.325527	6339.560207	8.220006	-0.045515	4.302575
220.520421	6347.617290	8.225011	-0.045557	4.305214
220.617758	6355.560487	8.230016	-0.045580	4.307814
220.890963	6363.683965	8.235021	-0.045637	4.310472
220.933617	6371.659288	8.240026	-0.045650	4.313079
221.197302	6379.687923	8.245030	-0.045705	4.315703
221.103994	6387.683778	8.250035	-0.045693	4.318312
221.214951	6395.695136	8.255040	-0.045719	4.320926
221.681721	6403.680425	8.260045	-0.045811	4.323532
221.730714	6411.730823	8.265050	-0.045826	4.326155
221.984181	6419.692427	8.270054	-0.045878	4.328749
222.142802	6427.783835	8.275059	-0.045913	4.331384
222.359998	6435.779098	8.280064	-0.045959	4.333985
222.327022	6443.827869	8.285069	-0.045959	4.336601
222.543131	6451.811778	8.290074	-0.046004	4.339195
222.717896	6459.856270	8.295078	-0.046042	4.341808
222.893659	6467.810362	8.300083	-0.046081	4.344389
223.000593	6475.878569	8.305088	-0.046106	4.347006
223.406389	6483.881954	8.310093	-0.046187	4.349602
223.471153	6491.977257	8.315098	-0.046205	4.352224
223.762558	6500.005372	8.320102	-0.046264	4.354824
223.668454	6508.011321	8.325107	-0.046252	4.357413
223.839995	6515.944306	8.330112	-0.046290	4.359978
223.695971	6523.976167	8.335117	-0.046268	4.362572
224.070964	6531.977584	8.340122	-0.046344	4.365157
224.495322	6539.969410	8.345126	-0.046428	4.367739
224.531941	6548.007375	8.350131	-0.046440	4.370331
224.426905	6556.022748	8.355136	-0.046426	4.372913
224.878359	6564.080022	8.360141	-0.046516	4.375511
225.121783	6572.074294	8.365146	-0.046567	4.378086
225.141235	6580.054144	8.370150	-0.046576	4.380653
225.388719	6588.086078	8.375155	-0.046627	4.383237
225.511875	6596.085217	8.380160	-0.046656	4.385808
225.726659	6604.110838	8.385165	-0.046701	4.388386
225.717044	6612.147117	8.390170	-0.046705	4.390965
225.872127	6620.186269	8.395174	-0.046739	4.393545
226.020979	6628.239091	8.400179	-0.046772	4.396127
226.109307	6636.151512	8.405184	-0.046794	4.398662
226.310759	6644.213942	8.410189	-0.046837	4.401245
226.583716	6652.205854	8.415194	-0.046893	4.403804
226.580647	6660.243133	8.420198	-0.046898	4.406374
226.937514	6668.273489	8.425203	-0.046970	4.408943
227.074781	6676.290642	8.430208	-0.047001	4.411504
227.089390	6684.336931	8.435213	-0.047010	4.414073
227.168172	6692.364420	8.440218	-0.047030	4.416635
227.393473	6700.304276	8.445222	-0.047077	4.419167
227.393142	6708.405046	8.450227	-0.047083	4.421749
227.611016	6716.371030	8.455232	-0.047129	4.424287
227.771613	6724.376859	8.460237	-0.047164	4.426836
227.948643	6732.410697	8.465242	-0.047202	4.429393
227.982128	6740.467999	8.470246	-0.047214	4.431955
228.024398	6748.508240	8.475251	-0.047227	4.434510
228.377230	6756.516386	8.480256	-0.047299	4.437055
228.642811	6764.504889	8.485261	-0.047353	4.439591
228.824941	6772.533656	8.490266	-0.047393	4.442139
228.975145	6780.484790	8.495270	-0.047426	4.444660
229.125551	6788.543009	8.500275	-0.047460	4.447214
229.088992	6796.522539	8.505280	-0.047458	4.449741
229.353937	6804.595526	8.510285	-0.047513	4.452297
229.705767	6812.650459	8.515290	-0.047584	4.454846
229.675990	6820.616057	8.520294	-0.047584	4.457364
229.920120	6828.633251	8.525299	-0.047635	4.459897
230.164445	6836.624446	8.530304	-0.047686	4.462421
230.359299	6844.625798	8.535309	-0.047728	4.464947
230.344512	6852.664878	8.540314	-0.047731	4.467483
230.740653	6860.672167	8.545318	-0.047810	4.470008
230.963135	6868.766380	8.550323	-0.047857	4.472559
230.784224	6876.735797	8.555328	-0.047829	4.475067
231.073756	6884.730393	8.560333	-0.047888	4.477584
231.313659	6892.735097	8.565338	-0.047938	4.480102
231.402807	6900.735040	8.570343	-0.047960	4.482617
231.505611	6908.793063	8.575347	-0.047985	4.485148
231.554654	6916.761729	8.580352	-0.048000	4.487650
231.928001	6924.784447	8.585357	-0.048075	4.490169
231.913958	6932.850389	8.590362	-0.048077	4.492698
231.957695	6940.875500	8.595367	-0.048091	4.495214
232.346369	6948.868067	8.600371	-0.048169	4.497719
232.445728	6956.824960	8.605376	-0.048193	4.500210
232.484097	6964.871681	8.610381	-0.048205	4.502728
232.572590	6972.886547	8.615386	-0.048227	4.505234
232.558975	6980.912775	8.620391	-0.048230	4.507743
233.017927	6988.938594	8.625395	-0.048321	4.510251
233.008437	6997.013839	8.630400	-0.048325	4.512772
233.340284	7005.036887	8.635405	-0.048392	4.515276
233.395765	7013.007553	8.640410	-0.048408	4.517762
233.493541	7020.975310	8.645415	-0.048432	4.520246
233.697331	7028.990838	8.650419	-0.048475	4.522743
233.558550	7036.984210	8.655424	-0.048455	4.525231
233.986855	7045.016188	8.660429	-0.048540	4.527731
234.115197	7053.030677	8.665434	-0.048569	4.530224
234.262947	7061.061572	8.670439	-0.048602	4.532720
234.507232	7069.094344	8.675443	-0.048653	4.535216
234.705377	7077.120861	8.680448	-0.048696	4.537708
234.825430	7085.085910	8.685453	-0.048723	4.540180
235.032040	7093.141465	8.690458	-0.048767	4.542678
234.787379	7101.116364	8.695463	-0.048727	4.545150
235.194017	7109.170699	8.700467	-0.048809	4.547646
235.202337	7117.165087	8.705472	-0.048816	4.550121
235.349088	7125.257016	8.710477	-0.048848	4.552625
235.324558	7133.265414	8.715482	-0.048849	4.555102
235.448540	7141.253251	8.720487	-0.048878	4.557571
235.633385	7149.262399	8.725491	-0.048918	4.560045
235.864935	7157.243418	8.730496	-0.048966	4.562510
236.001887	7165.245416	8.735501	-0.048997	4.564979
236.089462	7173.268193	8.740506	-0.049019	4.567454
236.198523	7181.275025	8.745511	-0.049045	4.569922
236.423578	7189.390254	8.750515	-0.049092	4.572422
236.574273	7197.395652	8.755520	-0.049126	4.574888
236.762469	7205.383000	8.760525	-0.049166	4.577346
237.011030	7213.354250	8.765530	-0.049218	4.579798
237.207704	7221.381819	8.770535	-0.049260	4.582266
237.267657	7229.407010	8.775539	-0.049277	4.584732
237.441609	7237.444441	8.780544	-0.049315	4.587200
237.639698	7245.449599	8.785549	-0.049357	4.589657
237.867883	7253.531360	8.790554	-0.049405	4.592136
237.878693	7261.547649	8.795559	-0.049412	4.594594
238.045360	7269.533373	8.800563	-0.049449	4.597041
238.123491	7277.507217	8.805568	-0.049469	4.599483
238.338754	7285.560696	8.810573	-0.049514	4.601948
238.540081	7293.516518	8.815578	-0.049557	4.604382
238.806347	7301.556260	8.820583	-0.049612	4.606840
238.937233	7309.562657	8.825587	-0.049642	4.609287
239.019125	7317.599961	8.830592	-0.049663	4.611742
239.322222	7325.610890	8.835597	-0.049725	4.614187
239.599555	7333.692723	8.840602	-0.049782	4.616653
239.676689	7341.577175	8.845607	-0.049802	4.619057
239.946327	7349.671829	8.850611	-0.049858	4.621524
240.041008	7357.647769	8.855616	-0.049881	4.623954
240.088208	7365.708937	8.860621	-0.049895	4.626408
240.191343	7373.709821	8.865626	-0.049920	4.628842
240.319993	7381.726293	8.870631	-0.049949	4.631280
240.392552	7389.772647	8.875635	-0.049968	4.633726
240.463691	7397.783198	8.880640	-0.049987	4.636160
240.756494	7405.726426	8.885645	-0.050047	4.638571
240.940810	7413.804363	8.890650	-0.050086	4.641023
240.897123	7421.776994	8.895655	-0.050084	4.643441
241.112178	7429.815194	8.900659	-0.050129	4.645878
241.599785	7437.820306	8.905664	-0.050226	4.648303
241.853741	7445.821904	8.910669	-0.050278	4.650726
241.881327	7453.887955	8.915674	-0.050289	4.653167
242.025444	7461.849223	8.920679	-0.050321	4.655576
242.163939	7469.904512	8.925683	-0.050352	4.658011
242.289807	7477.869998	8.930688	-0.050381	4.660418
242.443939	7485.933851	8.935693	-0.050416	4.662854
242.670098	7493.943319	8.940698	-0.050463	4.665271
242.713073	7501.924174	8.945703	-0.050477	4.667679
242.955661	7509.977370	8.950707	-0.050527	4.670108
243.025078	7518.068248	8.955712	-0.050546	4.672546
242.986740	7526.062316	8.960717	-0.050544	4.674955
243.241662	7534.072346	8.965722	-0.050597	4.677366
243.737043	7541.982030	8.970727	-0.050695	4.679746
243.820215	7550.095118	8.975731	-0.050716	4.682186
243.921339	7557.981976	8.980736	-0.050740	4.684557
244.267840	7566.032273	8.985741	-0.050810	4.686975
244.476547	7574.065247	8.990746	-0.050854	4.689387
244.389097	7582.078761	8.995751	-0.050843	4.691793
244.554654	7590.134412	9.000755	-0.050880	4.694209
244.922025	7598.172705	9.005760	-0.050954	4.696619
245.119869	7606.113052	9.010765	-0.050996	4.698998
245.281603	7614.153169	9.015770	-0.051031	4.701406
245.490289	7622.124800	9.020775	-0.051076	4.703792
245.427151	7630.175791	9.025779	-0.051069	4.706201
245.473266	7638.150276	9.030784	-0.051083	4.708586
245.519497	7646.256280	9.035789	-0.051098	4.711009
245.950416	7654.267113	9.040794	-0.051183	4.713401
246.017414	7662.278179	9.045799	-0.051201	4.715794
246.195294	7670.323568	9.050803	-0.051240	4.718194
246.332221	7678.280662	9.055808	-0.051271	4.720568
246.403659	7686.295711	9.060813	-0.051290	4.722957
246.407738	7694.341499	9.065818	-0.051296	4.725355
246.471338	7702.342651	9.070823	-0.051313	4.727738
246.725377	7710.358039	9.075827	-0.051366	4.730124
246.920991	7718.411656	9.080832	-0.051408	4.732519
246.957031	7726.390187	9.085837	-0.051420	4.734892
247.326142	7734.485299	9.090842	-0.051494	4.737297
247.319286	7742.384325	9.095847	-0.051498	4.739644
247.573214	7750.461368	9.100851	-0.051551	4.742042
247.752591	7758.460807	9.105856	-0.051590	4.744415
247.997846	7766.500825	9.110861	-0.051641	4.746800
248.030585	7774.486856	9.115866	-0.051653	4.749167
248.065619	7782.521176	9.120871	-0.051665	4.751548
248.421775	7790.560003	9.125875	-0.051736	4.753928
248.575009	7798.618609	9.130880	-0.051771	4.756313
248.828039	7806.517856	9.135885	-0.051823	4.758650
248.917653	7814.594429	9.140890	-0.051845	4.761038
248.944304	7822.508486	9.145895	-0.051856	4.763378
249.182103	7830.537899	9.150899	-0.051905	4.765749
249.404226	7838.562757	9.155904	-0.051952	4.768118
249.563578	7846.542238	9.160909	-0.051987	4.770473
249.552922	7854.681272	9.165914	-0.051991	4.772874
249.890839	7862.661616	9.170919	-0.052059	4.775226
250.197727	7870.690124	9.175923	-0.052122	4.777590
250.064378	7878.658525	9.180928	-0.052102	4.779938
249.999413	7886.647642	9.185933	-0.052096	4.782291
250.474649	7894.669352	9.190938	-0.052190	4.784649
250.576187	7902.677242	9.195943	-0.052214	4.787004
250.663990	7910.769657	9.200947	-0.052236	4.789383
250.717072	7918.737044	9.205952	-0.052251	4.791724
250.920034	7926.809426	9.210957	-0.052295	4.794094
250.998822	7934.812778	9.215962	-0.052315	4.796443
251.008582	7942.785000	9.220967	-0.052322	4.798782
251.432285	7950.806800	9.225971	-0.052406	4.801132
251.513994	7958.791226	9.230976	-0.052427	4.803472
251.498613	7966.820711	9.235981	-0.052430	4.805825
251.736769	7974.867724	9.240986	-0.052480	4.808180
251.933622	7982.851971	9.245991	-0.052522	4.810516
252.109005	7990.353066	9.250995	-0.052559	4.812709
252.218257	7994.884729	9.256000	-0.052583	4.814034

252.225436	7997.433808	9.261005	-0.052586	4.814779
252.237489	7998.747628	9.266010	-0.052590	4.815163
252.381352	7999.123808	9.271015	-0.052617	4.815272
252.722604	8000.148356	9.276019	-0.052681	4.815570
252.614853	8000.122047	9.281024	-0.052661	4.815563
252.766851	8000.150191	9.286029	-0.052690	4.815571
252.923239	8000.114320	9.291034	-0.052719	4.815559
252.909751	8000.117325	9.296039	-0.052717	4.815560
252.807651	8000.153060	9.301043	-0.052698	4.815571
253.023697	8000.138459	9.306048	-0.052739	4.815566
253.199972	8000.146707	9.311053	-0.052772	4.815567
253.176226	8000.146340	9.316058	-0.052768	4.815567
253.016018	8000.159761	9.321063	-0.052738	4.815572
253.105783	8000.153775	9.326067	-0.052755	4.815570
253.177892	8000.154977	9.331072	-0.052769	4.815570
253.167751	8000.160173	9.336077	-0.052767	4.815572
253.352831	8000.145066	9.341082	-0.052802	4.815566
253.171763	8000.137851	9.346087	-0.052768	4.815565
253.214232	8000.164203	9.351091	-0.052777	4.815572
253.247345	8000.131655	9.356096	-0.052783	4.815563
253.201403	8000.155491	9.361101	-0.052775	4.815570
253.034578	8000.150646	9.366106	-0.052744	4.815569
253.030593	8000.148466	9.371111	-0.052743	4.815569
253.441868	8000.148811	9.376115	-0.052820	4.815567
253.519374	8000.142624	9.381120	-0.052835	4.815565
253.409662	8000.152600	9.386125	-0.052815	4.815568
253.307172	8000.149875	9.391130	-0.052796	4.815568
253.440035	8000.136050	9.396135	-0.052821	4.815563
253.722093	8000.168461	9.401139	-0.052874	4.815571
253.710870	8000.130914	9.406144	-0.052872	4.815560
253.767728	8000.140411	9.411149	-0.052883	4.815563
253.822428	8000.153078	9.416154	-0.052893	4.815566
253.602760	8000.148435	9.421159	-0.052852	4.815566
253.510240	8000.164032	9.426163	-0.052835	4.815571
253.610080	8000.131508	9.431168	-0.052854	4.815561
253.619687	8000.160527	9.436173	-0.052856	4.815569
253.737210	8000.150723	9.441178	-0.052878	4.815566
253.665420	8000.142092	9.446183	-0.052865	4.815564
253.677299	8000.158330	9.451187	-0.052868	4.815568
253.584390	8000.135468	9.456192	-0.052851	4.815562
253.747645	8000.180888	9.461197	-0.052881	4.815575
253.812583	8000.164883	9.466202	-0.052894	4.815570
253.676379	8000.139175	9.471207	-0.052868	4.815563
254.013409	8000.176759	9.476211	-0.052931	4.815572
253.979641	8000.135638	9.481216	-0.052925	4.815560
253.944508	8000.147902	9.486221	-0.052919	4.815564
253.896418	8000.156750	9.491226	-0.052910	4.815567
254.020336	8000.131029	9.496231	-0.052934	4.815559
253.994293	8000.165873	9.501235	-0.052929	4.815569
253.944250	8000.134099	9.506240	-0.052920	4.815560
254.060183	8000.166995	9.511245	-0.052942	4.815569
254.090182	8000.163235	9.516250	-0.052948	4.815568
253.982820	8000.152954	9.521255	-0.052928	4.815565
253.977439	8000.197750	9.526259	-0.052927	4.815578
254.175004	8000.156144	9.531264	-0.052964	4.815565
254.096010	8000.177303	9.536269	-0.052950	4.815572
254.344023	8000.176046	9.541274	-0.052996	4.815570
254.048568	8000.162684	9.546279	-0.052941	4.815568
254.424496	8000.179543	9.551283	-0.053012	4.815571
254.197493	8000.144871	9.556288	-0.052970	4.815562
254.335476	8000.180265	9.561293	-0.052996	4.815572
254.526200	8000.184478	9.566298	-0.053031	4.815572
254.286324	8000.167753	9.571303	-0.052987	4.815568
254.478219	8000.181599	9.576307	-0.053023	4.815571
254.616557	8000.175341	9.581312	-0.053049	4.815569
254.450294	8000.189730	9.586317	-0.053018	4.815574
254.572274	8000.178932	9.591322	-0.053041	4.815570
254.423207	8000.175444	9.596327	-0.053014	4.815570
254.578143	8000.187617	9.601331	-0.053043	4.815572
254.253119	8000.194065	9.606336	-0.052983	4.815576
254.518276	8000.219793	9.611341	-0.053032	4.815582
254.559061	8000.195914	9.616346	-0.053040	4.815575
254.360231	8000.188407	9.621351	-0.053003	4.815574
254.411973	8000.199958	9.626355	-0.053013	4.815577
254.521536	8000.151570	9.631360	-0.053034	4.815562
254.306258	8000.187588	9.636365	-0.052994	4.815574
254.568159	8000.215399	9.641370	-0.053043	4.815581
254.574638	8000.165323	9.646375	-0.053044	4.815566
254.544111	8000.208639	9.651379	-0.053039	4.815579
254.435746	8000.163091	9.656384	-0.053019	4.815566
254.546522	8000.187358	9.661389	-0.053040	4.815572
254.590098	8000.211593	9.666394	-0.053048	4.815579
254.484724	8000.172503	9.671399	-0.053029	4.815568
254.609544	8000.203410	9.676403	-0.053052	4.815577
254.726218	8000.181843	9.681408	-0.053074	4.815570
254.712906	8000.194465	9.686413	-0.053072	4.815574
254.591563	8000.181817	9.691418	-0.053050	4.815571
254.621738	8000.180196	9.696423	-0.053056	4.815570
254.786651	8000.216033	9.701427	-0.053087	4.815580
254.545880	8000.185406	9.706432	-0.053042	4.815572
254.502618	8000.192196	9.711437	-0.053034	4.815574
254.740425	8000.202522	9.716442	-0.053079	4.815576
254.587395	8000.163720	9.721447	-0.053050	4.815565
254.589064	8000.200086	9.726451	-0.053051	4.815576
254.751735	8000.165386	9.731456	-0.053081	4.815565
254.693485	8000.180477	9.736461	-0.053071	4.815570
254.784444	8000.177715	9.741466	-0.053088	4.815568
254.795507	8000.172577	9.746471	-0.053090	4.815567
254.965843	8000.223457	9.751475	-0.053122	4.815581
254.842841	8000.160578	9.756480	-0.053100	4.815563
254.970843	8000.188333	9.761485	-0.053124	4.815571
255.123552	8000.200470	9.766490	-0.053152	4.815573
254.800747	8000.156749	9.771495	-0.053093	4.815562
254.724418	8000.172611	9.776499	-0.053079	4.815567
254.816881	8000.181624	9.781504	-0.053096	4.815569
254.997490	8000.186741	9.786509	-0.053130	4.815570
255.001195	8000.195369	9.791514	-0.053131	4.815572
254.898848	8000.174487	9.796519	-0.053112	4.815567
255.067051	8000.191150	9.801523	-0.053144	4.815571
254.955407	8000.176525	9.806528	-0.053123	4.815567
254.837372	8000.191703	9.811533	-0.053101	4.815572
255.105598	8000.193983	9.816538	-0.053152	4.815572
255.073982	8000.159305	9.821543	-0.053146	4.815562
255.049930	8000.224091	9.826547	-0.053142	4.815581
254.967919	8000.178974	9.831552	-0.053127	4.815568
254.983817	8000.169643	9.836557	-0.053130	4.815565
255.045829	8000.181362	9.841562	-0.053142	4.815568
254.893296	8000.187430	9.846567	-0.053114	4.815571
254.923823	8000.197565	9.851571	-0.053119	4.815573
255.041047	8000.198439	9.856576	-0.053142	4.815573
254.978160	8000.191022	9.861581	-0.053130	4.815571
255.241689	8000.202838	9.866586	-0.053179	4.815573
255.192080	8000.159319	9.871591	-0.053170	4.815561
255.076672	8000.202314	9.876595	-0.053149	4.815574
255.070175	8000.176593	9.881600	-0.053148	4.815567
255.060509	8000.195683	9.886605	-0.053147	4.815572
255.104475	8000.198562	9.891610	-0.053155	4.815573
255.188230	8000.165774	9.896615	-0.053171	4.815563
255.258048	8000.185098	9.901619	-0.053184	4.815568
255.192684	8000.166958	9.906624	-0.053172	4.815563
255.163654	8000.186800	9.911629	-0.053167	4.815569
255.327040	8000.217271	9.916634	-0.053198	4.815577
255.365976	8000.197635	9.921639	-0.053205	4.815571
255.433748	8000.195563	9.926643	-0.053218	4.815570
255.239768	8000.187065	9.931648	-0.053182	4.815569
255.153532	8000.188878	9.936653	-0.053166	4.815570
255.210731	8000.190905	9.941658	-0.053177	4.815570
255.053494	8000.163783	9.946663	-0.053148	4.815563
255.119443	8000.203339	9.951667	-0.053161	4.815574
255.337491	8000.200524	9.956672	-0.053202	4.815572
255.266913	8000.219685	9.961677	-0.053189	4.815578
255.477674	8000.217819	9.966682	-0.053228	4.815577
255.304681	8000.178688	9.971687	-0.053196	4.815566
255.268253	8000.209090	9.976691	-0.053190	4.815575
255.226877	8000.186002	9.981696	-0.053182	4.815568
255.172609	8000.186203	9.986701	-0.053172	4.815569
255.143770	8000.188956	9.991706	-0.053167	4.815570
255.134298	8000.182414	9.996711	-0.053166	4.815568
255.454895	8000.199438	10.001715	-0.053226	4.815571
255.527726	8000.181426	10.006720	-0.053240	4.815566
255.143108	8000.193305	10.011725	-0.053168	4.815571
255.353683	8000.192504	10.016730	-0.053208	4.815570
255.406829	8000.177374	10.021735	-0.053218	4.815565
255.332026	8000.191124	10.026739	-0.053204	4.815569
255.328590	8000.166521	10.031744	-0.053204	4.815562
255.248810	8000.195145	10.036749	-0.053189	4.815571
255.526351	8000.208260	10.041754	-0.053241	4.815573
255.394394	8000.174073	10.046759	-0.053217	4.815564
255.443539	8000.194128	10.051763	-0.053226	4.815570
255.310897	8000.175953	10.056768	-0.053202	4.815565
255.249443	8000.170695	10.061773	-0.053190	4.815564
255.415112	8000.207613	10.066778	-0.053222	4.815574
255.358303	8000.192818	10.071783	-0.053211	4.815570
255.457956	8000.206222	10.076787	-0.053230	4.815573
255.554405	8000.191802	10.081792	-0.053248	4.815568
255.400559	8000.191439	10.086797	-0.053220	4.815569
255.594419	8000.197841	10.091802	-0.053256	4.815570
255.258060	8000.194488	10.096807	-0.053194	4.815571
255.492799	8000.213311	10.101811	-0.053238	4.815575
255.372694	8000.176114	10.106816	-0.053216	4.815565
255.171210	8000.193130	10.111821	-0.053178	4.815571
255.555163	8000.207988	10.116826	-0.053250	4.815573
255.417592	8000.205756	10.121831	-0.053225	4.815573
255.695249	8000.238100	10.126835	-0.053277	4.815581
255.615053	8000.183398	10.131840	-0.053262	4.815566
255.413251	8000.201477	10.136845	-0.053225	4.815572
255.605686	8000.233493	10.141850	-0.053261	4.815580
255.638687	8000.195600	10.146855	-0.053267	4.815569
255.592203	8000.224770	10.151859	-0.053259	4.815578
255.556115	8000.217791	10.156864	-0.053252	4.815576
255.582723	8000.194748	10.161869	-0.053257	4.815569
255.547844	8000.194198	10.166874	-0.053251	4.815569
255.457731	8000.188471	10.171879	-0.053235	4.815568
255.643748	8000.212904	10.176883	-0.053270	4.815574
255.649695	8000.194864	10.181888	-0.053271	4.815569
255.532752	8000.204720	10.186893	-0.053249	4.815572
255.539646	8000.208059	10.191898	-0.053251	4.815573
255.402423	8000.226127	10.196903	-0.053226	4.815579
255.503165	8000.235277	10.201907	-0.053245	4.815581
255.500725	8000.180781	10.206912	-0.053244	4.815565
255.717613	8000.187561	10.211917	-0.053285	4.815566
255.609548	8000.206108	10.216922	-0.053265	4.815572
255.656687	8000.178061	10.221927	-0.053274	4.815564
255.761067	8000.195816	10.226931	-0.053294	4.815568
255.621382	8000.206367	10.231936	-0.053268	4.815572
255.673005	8000.214712	10.236941	-0.053278	4.815574
255.873549	8000.227634	10.241946	-0.053315	4.815577
255.877726	8000.206360	10.246951	-0.053317	4.815571
255.776707	8000.232499	10.251955	-0.053298	4.815579
255.862296	8000.199741	10.256960	-0.053314	4.815569
255.808634	8000.206361	10.261965	-0.053304	4.815571
255.861705	8000.227548	10.266970	-0.053315	4.815577
255.796618	8000.205139	10.271975	-0.053303	4.815571
255.730070	8000.195524	10.276979	-0.053290	4.815568
255.780462	8000.181417	10.281984	-0.053300	4.815564
255.652034	8000.224198	10.286989	-0.053276	4.815577
255.798744	8000.221283	10.291994	-0.053304	4.815576
255.733825	8000.188195	10.296999	-0.053292	4.815566
255.817587	8000.220567	10.302003	-0.053308	4.815575
255.914037	8000.176237	10.307008	-0.053326	4.815562
255.946952	8000.207776	10.312013	-0.053333	4.815571
256.032915	8000.210275	10.317018	-0.053349	4.815571
255.750113	8000.197116	10.322023	-0.053296	4.815569
255.994028	8000.213954	10.327027	-0.053342	4.815572
255.765139	8000.194201	10.332032	-0.053300	4.815568
255.585047	8000.214771	10.337037	-0.053266	4.815575
255.804225	8000.233340	10.342042	-0.053308	4.815579
255.754661	8000.206912	10.347047	-0.053299	4.815572
255.825033	8000.232656	10.352051	-0.053312	4.815579
255.792269	8000.219322	10.357056	-0.053306	4.815575
255.847832	8000.232005	10.362061	-0.053317	4.815578
255.781083	8000.227728	10.367066	-0.053304	4.815577
255.667774	8000.142573	10.372071	-0.053284	4.815553
255.735737	8000.190709	10.377075	-0.053296	4.815567
255.769953	8000.179541	10.382080	-0.053303	4.815563
255.810241	8000.193042	10.387085	-0.053311	4.815567
255.879857	8000.202750	10.392090	-0.053324	4.815570
255.714248	8000.194716	10.397095	-0.053293	4.815568
255.905658	8000.220307	10.402099	-0.053329	4.815575
255.998660	8000.210103	10.407104	-0.053347	4.815571
255.997542	8000.212243	10.412109	-0.053347	4.815572
255.927001	8000.220722	10.417114	-0.053334	4.815575
255.677327	8000.158969	10.422119	-0.053288	4.815558
255.907747	8000.191608	10.427123	-0.053331	4.815566
255.915595	8000.184281	10.432128	-0.053333	4.815564
255.635570	8000.178645	10.437133	-0.053281	4.815564
255.815321	8000.196568	10.442138	-0.053314	4.815568
255.842802	8000.208790	10.447143	-0.053320	4.815572
255.873962	8000.240300	10.452147	-0.053326	4.815581
255.886955	8000.237330	10.457152	-0.053329	4.815580
255.619160	8000.218008	10.462157	-0.053279	4.815575
255.844981	8000.217458	10.467162	-0.053321	4.815574
255.924657	8000.182466	10.472167	-0.053336	4.815563
256.007563	8000.212688	10.477171	-0.053352	4.815572
255.680162	8000.209481	10.482176	-0.053291	4.815572
255.779935	8000.203660	10.487181	-0.053310	4.815570
255.957247	8000.215133	10.492186	-0.053343	4.815573
255.852448	8000.191005	10.497191	-0.053324	4.815566
255.987325	8000.230625	10.502195	-0.053349	4.815577
255.932697	8000.213728	10.507200	-0.053340	4.815572
255.881273	8000.187270	10.512205	-0.053330	4.815565
255.920557	8000.217845	10.517210	-0.053338	4.815574
255.689625	8000.160672	10.522215	-0.053295	4.815558
255.816597	8000.205502	10.527219	-0.053319	4.815571
255.894394	8000.198253	10.532224	-0.053334	4.815568
255.886633	8000.197080	10.537229	-0.053332	4.815568
256.155514	8000.214327	10.542234	-0.053383	4.815572
256.032295	8000.176010	10.547239	-0.053360	4.815561
256.010436	8000.205583	10.552243	-0.053356	4.815570
255.841092	8000.171851	10.557248	-0.053325	4.815561
255.920039	8000.173167	10.562253	-0.053340	4.815561
255.986852	8000.190306	10.567258	-0.053353	4.815565
255.981175	8000.162462	10.572263	-0.053352	4.815557
255.983174	8000.187085	10.577267	-0.053352	4.815564
255.908086	8000.199762	10.582272	-0.053339	4.815568
255.948665	8000.182290	10.587277	-0.053346	4.815563
256.016336	8000.216535	10.592282	-0.053359	4.815573
255.962475	8000.190037	10.597287	-0.053349	4.815565
256.009334	8000.212191	10.602291	-0.053358	4.815572
255.930104	8000.188481	10.607296	-0.053344	4.815565
255.899772	8000.206165	10.612301	-0.053339	4.815570
256.110088	8000.219248	10.617306	-0.053378	4.815573
255.880637	8000.195213	10.622311	-0.053335	4.815567
255.909694	8000.221348	10.627315	-0.053341	4.815575
256.075636	8000.202725	10.632320	-0.053372	4.815568
255.929461	8000.188601	10.637325	-0.053345	4.815565
255.870324	8000.210085	10.642330	-0.053335	4.815572
255.963712	8000.179591	10.647335	-0.053352	4.815562
255.912857	8000.192666	10.652339	-0.053343	4.815566
255.948458	8000.182589	10.657344	-0.053350	4.815563
256.143490	8000.206104	10.662349	-0.053386	4.815569
256.185027	8000.199329	10.667354	-0.053394	4.815567
256.185686	8000.157701	10.672359	-0.053395	4.815555
256.055814	8000.201527	10.677363	-0.053371	4.815568
255.804901	8000.201709	10.682368	-0.053324	4.815569
255.719271	8000.187509	10.687373	-0.053309	4.815566
255.950922	8000.205214	10.692378	-0.053352	4.815570
256.055687	8000.202680	10.697383	-0.053372	4.815568
255.903409	8000.233320	10.702387	-0.053344	4.815578
255.948809	8000.215926	10.707392	-0.053352	4.815573
255.938861	8000.195489	10.712397	-0.053351	4.815567
255.992696	8000.215620	10.717402	-0.053361	4.815572
256.002632	8000.210464	10.722407	-0.053363	4.815571
256.132715	8000.220095	10.727411	-0.053388	4.815573
256.244430	8000.215539	10.732416	-0.053409	4.815571
256.175405	8000.225111	10.737421	-0.053396	4.815574
256.088368	8000.231184	10.742426	-0.053380	4.815577
256.059121	8000.200816	10.747431	-0.053375	4.815568
256.044953	8000.233720	10.752435	-0.053373	4.815577
256.135624	8000.223478	10.757440	-0.053390	4.815574
256.094271	8000.208935	10.762445	-0.053382	4.815570
256.151387	8000.204551	10.767450	-0.053393	4.815568
255.997372	8000.170002	10.772455	-0.053365	4.815559
255.881643	8000.200173	10.777459	-0.053343	4.815568
256.079650	8000.211986	10.782464	-0.053380	4.815571
255.976191	8000.179334	10.787469	-0.053361	4.815562
256.265902	8000.225765	10.792474	-0.053416	4.815574
256.236884	8000.205015	10.797479	-0.053410	4.815568
256.220477	8000.211177	10.802483	-0.053408	4.815570
256.093056	8000.190950	10.807488	-0.053384	4.815565
256.123373	8000.216037	10.812493	-0.053390	4.815572
256.356612	8000.236974	10.817498	-0.053434	4.815577
256.293077	8000.227408	10.822503	-0.053422	4.815574
256.133598	8000.234430	10.827507	-0.053393	4.815577
256.204046	8000.238811	10.832512	-0.053406	4.815578
256.111459	8000.221291	10.837517	-0.053389	4.815573
256.115636	8000.259837	10.842522	-0.053390	4.815585
256.177737	8000.208534	10.847527	-0.053402	4.815569
256.248675	8000.222538	10.852531	-0.053415	4.815573
256.234585	8000.225533	10.857536	-0.053413	4.815574
256.133832	8000.220698	10.862541	-0.053394	4.815573
256.336188	8000.262493	10.867546	-0.053432	4.815584
255.998271	8000.195019	10.872551	-0.053370	4.815566
256.125135	8000.233439	10.877555	-0.053394	4.815577
256.302484	8000.234232	10.882560	-0.053427	4.815576
256.236498	8000.198989	10.887565	-0.053415	4.815566
256.419944	8000.224450	10.892570	-0.053449	4.815573
256.371423	8000.176675	10.897575	-0.053440	4.815559
256.305366	8000.206592	10.902579	-0.053428	4.815568
256.293533	8000.193601	10.907584	-0.053426	4.815564
256.335684	8000.206064	10.912589	-0.053434	4.815568
256.535854	8000.221118	10.917594	-0.053472	4.815571
256.193559	8000.199505	10.922599	-0.053409	4.815567
256.215250	8000.196677	10.927603	-0.053413	4.815566
256.300836	8000.209852	10.932608	-0.053429	4.815569
256.430697	8000.185297	10.937613	-0.053453	4.815561
256.381047	8000.205869	10.942618	-0.053444	4.815567
256.295986	8000.186337	10.947623	-0.053429	4.815562
256.507559	8000.206919	10.952627	-0.053468	4.815567
256.489446	8000.199166	10.957632	-0.053465	4.815565
256.298378	8000.189646	10.962637	-0.053430	4.815563
256.276433	8000.206399	10.967642	-0.053426	4.815568
256.285729	8000.196959	10.972647	-0.053428	4.815565
256.238328	8000.196204	10.977651	-0.053420	4.815565
256.488089	8000.197115	10.982656	-0.053466	4.815564
256.372276	8000.176010	10.987661	-0.053445	4.815559
256.516150	8000.227529	10.992666	-0.053472	4.815573
256.296691	8000.170542	10.997671	-0.053431	4.815557
256.475803	8000.221570	11.002675	-0.053465	4.815572
256.385346	8000.216904	11.007680	-0.053448	4.815571
256.183963	8000.197601	11.012685	-0.053411	4.815566
256.397019	8000.206456	11.017690	-0.053451	4.815567
256.297632	8000.163188	11.022695	-0.053433	4.815555
256.281267	8000.194988	11.027699	-0.053430	4.815565
256.472810	8000.204559	11.032704	-0.053466	4.815567
256.492470	8000.220926	11.037709	-0.053470	4.815571
256.290874	8000.217643	11.042714	-0.053433	4.815571
256.293284	8000.177112	11.047719	-0.053433	4.815559
256.490202	8000.170748	11.052723	-0.053470	4.815557
256.472636	8000.186505	11.057728	-0.053467	4.815561
256.447955	8000.176508	11.062733	-0.053463	4.815558
256.383253	8000.231016	11.067738	-0.053451	4.815575
256.569306	8000.214860	11.072743	-0.053486	4.815569
256.286385	8000.228403	11.077747	-0.053433	4.815574
256.442237	8000.218161	11.082752	-0.053463	4.815571
256.345504	8000.195233	11.087757	-0.053445	4.815564
256.309457	8000.213891	11.092762	-0.053438	4.815570
256.103494	8000.163535	11.097767	-0.053400	4.815556
256.297021	8000.197707	11.102771	-0.053437	4.815565
256.346440	8000.207085	11.107776	-0.053446	4.815568
256.415604	8000.218923	11.112781	-0.053459	4.815571
256.587425	8000.227103	11.117786	-0.053491	4.815572
256.587623	8000.167307	11.122791	-0.053492	4.815555
256.394235	8000.191932	11.127795	-0.053456	4.815563
256.265339	8000.196250	11.132800	-0.053432	4.815565
256.479076	8000.190161	11.137805	-0.053472	4.815562
256.632896	8000.221547	11.142810	-0.053501	4.815571
256.395082	8000.184555	11.147815	-0.053457	4.815561
256.463253	8000.217741	11.152819	-0.053470	4.815570
256.629693	8000.221560	11.157824	-0.053501	4.815571
256.401324	8000.172972	11.162829	-0.053459	4.815557
256.391868	8000.199544	11.167834	-0.053457	4.815565
256.482498	8000.201051	11.172839	-0.053475	4.815565
256.398754	8000.216792	11.177843	-0.053459	4.815570
256.385480	8000.188822	11.182848	-0.053457	4.815562
256.372138	8000.195034	11.187853	-0.053455	4.815564
256.219920	8000.238494	11.192858	-0.053427	4.815577
256.194401	8000.198573	11.197863	-0.053422	4.815566
256.438530	8000.244258	11.202867	-0.053468	4.815578
256.661977	8000.210555	11.207872	-0.053510	4.815567
256.504407	8000.218675	11.212877	-0.053481	4.815570
256.695555	8000.251742	11.217882	-0.053517	4.815579
256.541940	8000.200106	11.222887	-0.053488	4.815565
256.520455	8000.212594	11.227891	-0.053484	4.815568
256.306008	8000.213373	11.232896	-0.053445	4.815570
256.499708	8000.205888	11.237901	-0.053481	4.815567
256.555447	8000.205755	11.242906	-0.053492	4.815566
256.327367	8000.179605	11.247911	-0.053449	4.815560
256.363294	8000.181284	11.252915	-0.053456	4.815560
256.499506	8000.168583	11.257920	-0.053482	4.815556
256.341978	8000.157477	11.262925	-0.053453	4.815553
256.500461	8000.233804	11.267930	-0.053483	4.815575
256.745061	8000.204721	11.272935	-0.053528	4.815565
256.610361	8000.205739	11.277939	-0.053504	4.815566
256.543747	8000.222828	11.282944	-0.053491	4.815571
256.572238	8000.208362	11.287949	-0.053497	4.815567
256.641776	8000.225547	11.292954	-0.053510	4.815572
256.610455	8000.196213	11.297959	-0.053505	4.815563
256.585696	8000.231080	11.302963	-0.053500	4.815573
256.804350	8000.234687	11.307968	-0.053541	4.815573
256.672947	8000.199439	11.312973	-0.053517	4.815564
256.729308	8000.231364	11.317978	-0.053528	4.815573
256.815136	8000.190063	11.322983	-0.053544	4.815560
256.692977	8000.245766	11.327987	-0.053521	4.815577
256.621602	8000.223253	11.332992	-0.053508	4.815571
256.537563	8000.218692	11.337997	-0.053493	4.815570
256.675313	8000.230587	11.343002	-0.053519	4.815573
256.446387	8000.214036	11.348007	-0.053477	4.815569
256.401141	8000.226134	11.353011	-0.053468	4.815573
256.770479	8000.239690	11.358016	-0.053537	4.815575
256.578243	8000.189557	11.363021	-0.053502	4.815561
256.588977	8000.248507	11.368026	-0.053504	4.815578
256.479695	8000.217895	11.373031	-0.053484	4.815570
256.544229	8000.220043	11.378035	-0.053496	4.815570
256.714760	8000.215383	11.383040	-0.053528	4.815568
256.379991	8000.206711	11.388045	-0.053466	4.815567
256.637315	8000.239794	11.393050	-0.053514	4.815576
256.588390	8000.187739	11.398055	-0.053505	4.815561
256.646237	8000.221824	11.403059	-0.053516	4.815570
256.475299	8000.216906	11.408064	-0.053485	4.815570
256.553688	8000.182962	11.413069	-0.053500	4.815559
256.606815	8000.225515	11.418074	-0.053510	4.815572
256.547981	8000.205344	11.423079	-0.053499	4.815566
256.670219	8000.225530	11.428083	-0.053522	4.815571
256.583400	8000.229469	11.433088	-0.053506	4.815573
256.559823	8000.203467	11.438093	-0.053502	4.815565
256.791407	8000.240401	11.443098	-0.053545	4.815575
256.659914	8000.200878	11.448103	-0.053521	4.815564
256.538439	8000.218136	11.453107	-0.053499	4.815570
256.704857	8000.228364	11.458112	-0.053530	4.815572
256.546871	8000.220454	11.463117	-0.053501	4.815570
256.737659	8000.236423	11.468122	-0.053537	4.815574
256.567432	8000.208016	11.473127	-0.053505	4.815567
256.633288	8000.236892	11.478131	-0.053518	4.815575
256.671415	8000.216174	11.483136	-0.053525	4.815568
256.659492	8000.228819	11.488141	-0.053523	4.815572
256.801708	8000.237582	11.493146	-0.053550	4.815574
256.607204	8000.184207	11.498151	-0.053514	4.815559
256.686652	8000.206896	11.503155	-0.053529	4.815566
256.804328	8000.213120	11.508160	-0.053551	4.815567
256.771724	8000.213676	11.513165	-0.053545	4.815567
256.526290	8000.227833	11.518170	-0.053500	4.815572
256.522540	8000.195746	11.523175	-0.053499	4.815563
256.728934	8000.214107	11.528179	-0.053538	4.815567
256.740603	8000.230344	11.533184	-0.053540	4.815572
256.635296	8000.194455	11.538189	-0.053521	4.815562
256.873092	8000.245379	11.543194	-0.053566	4.815576
256.882834	8000.198557	11.548199	-0.053568	4.815562
256.505776	8000.221239	11.553203	-0.053498	4.815571
256.596260	8000.212062	11.558208	-0.053515	4.815567
256.742936	8000.196328	11.563213	-0.053542	4.815562
256.794349	8000.242059	11.568218	-0.053552	4.815575
256.534282	8000.222861	11.573223	-0.053504	4.815571
256.678070	8000.224172	11.578227	-0.053531	4.815571
256.732952	8000.244322	11.583232	-0.053541	4.815576
256.515867	8000.235443	11.588237	-0.053501	4.815575
256.683527	8000.249964	11.593242	-0.053533	4.815578
256.620980	8000.205163	11.598247	-0.053521	4.815565
256.609098	8000.221013	11.603251	-0.053519	4.815570
256.616639	8000.233977	11.608256	-0.053521	4.815574
256.743829	8000.201901	11.613261	-0.053545	4.815564
256.820485	8000.236295	11.618266	-0.053559	4.815573
256.879540	8000.209511	11.623271	-0.053571	4.815565
256.887118	8000.211793	11.628275	-0.053572	4.815566
256.805317	8000.248930	11.633280	-0.053557	4.815577
256.600806	8000.225301	11.638285	-0.053520	4.815571
256.794420	8000.242385	11.643290	-0.053556	4.815575
257.121222	8000.245630	11.648295	-0.053617	4.815575
256.814981	8000.244902	11.653299	-0.053560	4.815576
256.770686	8000.224969	11.658304	-0.053552	4.815570
256.886914	8000.210873	11.663309	-0.053574	4.815566
257.020020	8000.217351	11.668314	-0.053599	4.815567
256.774350	8000.209071	11.673319	-0.053554	4.815566
256.658508	8000.226421	11.678323	-0.053532	4.815571
256.744438	8000.208623	11.683328	-0.053548	4.815566
256.755991	8000.205630	11.688333	-0.053551	4.815565
256.787453	8000.232873	11.693338	-0.053557	4.815572
256.996560	8000.194663	11.698343	-0.053596	4.815560
256.894363	8000.213305	11.703347	-0.053577	4.815566
256.970255	8000.226322	11.708352	-0.053592	4.815570
256.838935	8000.204962	11.713357	-0.053568	4.815564
256.858990	8000.250178	11.718362	-0.053572	4.815577
256.862033	8000.231022	11.723367	-0.053572	4.815572
257.038458	8000.218981	11.728371	-0.053605	4.815567
256.912736	8000.229760	11.733376	-0.053582	4.815571
256.893784	8000.199560	11.738381	-0.053579	4.815562
256.966092	8000.241361	11.743386	-0.053593	4.815574
256.958038	8000.196384	11.748391	-0.053591	4.815561
256.940954	8000.231378	11.753395	-0.053589	4.815571
256.904567	8000.242553	11.758400	-0.053582	4.815575
256.847529	8000.195705	11.763405	-0.053572	4.815561
257.055315	8000.227977	11.768410	-0.053611	4.815570
257.011626	8000.192030	11.773415	-0.053603	4.815559
256.936921	8000.200441	11.778419	-0.053589	4.815562
256.972867	8000.204257	11.783424	-0.053596	4.815563
257.174661	8000.234294	11.788429	-0.053634	4.815571
256.982781	8000.224759	11.793434	-0.053598	4.815569
256.967527	8000.193552	11.798439	-0.053596	4.815560
256.937300	8000.203760	11.803443	-0.053590	4.815563
257.124046	8000.236755	11.808448	-0.053625	4.815572
257.125708	8000.207962	11.813453	-0.053626	4.815563
257.177290	8000.213102	11.818458	-0.053636	4.815565
256.895329	8000.183930	11.823463	-0.053583	4.815557
256.984556	8000.219599	11.828467	-0.053600	4.815567
257.210833	8000.215854	11.833472	-0.053643	4.815565
256.889956	8000.197794	11.838477	-0.053583	4.815562
256.859504	8000.227227	11.843482	-0.053578	4.815570
256.999755	8000.213525	11.848487	-0.053604	4.815566
257.179660	8000.232521	11.853491	-0.053638	4.815570
257.125160	8000.224171	11.858496	-0.053628	4.815568
257.107155	8000.207874	11.863501	-0.053625	4.815563
257.115800	8000.227266	11.868506	-0.053627	4.815569
256.931603	8000.223198	11.873511	-0.053593	4.815569
256.890766	8000.210800	11.878515	-0.053585	4.815565
257.162120	8000.217408	11.883520	-0.053636	4.815566
257.167203	8000.184397	11.888525	-0.053637	4.815556
257.051705	8000.223118	11.893530	-0.053616	4.815568
256.906047	8000.196181	11.898535	-0.053589	4.815561
256.953460	8000.217277	11.903539	-0.053598	4.815567
256.948528	8000.238583	11.908544	-0.053598	4.815573
256.921878	8000.169800	11.913549	-0.053593	4.815553
256.810512	8000.203247	11.918554	-0.053572	4.815563
256.770850	8000.191936	11.923559	-0.053565	4.815560
256.811152	8000.186209	11.928563	-0.053573	4.815558
256.968165	8000.218717	11.933568	-0.053602	4.815567
256.888875	8000.189664	11.938573	-0.053588	4.815559
257.020132	8000.230295	11.943578	-0.053613	4.815570
256.987813	8000.202012	11.948583	-0.053607	4.815562
257.000133	8000.211850	11.953587	-0.053609	4.815565
257.229304	8000.264770	11.958592	-0.053652	4.815579
256.969607	8000.229553	11.963597	-0.053604	4.815570
257.224596	8000.226279	11.968602	-0.053652	4.815568
257.182906	8000.218139	11.973607	-0.053644	4.815566
256.990430	8000.213935	11.978611	-0.053609	4.815566
257.085862	8000.220864	11.983616	-0.053627	4.815567
257.065877	8000.186374	11.988621	-0.053623	4.815557
256.842729	8000.217988	11.993626	-0.053582	4.815567
256.818939	8000.185572	11.998631	-0.053578	4.815558
256.815324	8000.204763	12.003635	-0.053577	4.815564
256.819493	8000.223013	12.008640	-0.053578	4.815569
256.878440	8000.182340	12.013645	-0.053590	4.815557
256.752056	8000.210200	12.018650	-0.053566	4.815566
256.784304	8000.192590	12.023655	-0.053573	4.815560
256.767430	8000.175243	12.028659	-0.053570	4.815555
256.867150	8000.229244	12.033664	-0.053589	4.815571
256.798387	8000.178999	12.038669	-0.053576	4.815556
256.886431	8000.230672	12.043674	-0.053593	4.815571
256.929353	8000.224988	12.048679	-0.053601	4.815569
256.954199	8000.226485	12.053683	-0.053606	4.815569
257.069926	8000.220927	12.058688	-0.053628	4.815567
256.833814	8000.198916	12.063693	-0.053584	4.815562
257.076318	8000.229621	12.068698	-0.053629	4.815570
257.189178	8000.204788	12.073703	-0.053650	4.815562
257.142713	8000.213662	12.078707	-0.053642	4.815565
257.161373	8000.231081	12.083712	-0.053646	4.815570
256.977845	8000.185363	12.088717	-0.053612	4.815557
256.775138	8000.222654	12.093722	-0.053574	4.815569
257.054673	8000.227260	12.098727	-0.053627	4.815569
257.049674	8000.215449	12.103731	-0.053626	4.815566
257.306283	8000.213270	12.108736	-0.053674	4.815564
256.950796	8000.195710	12.113741	-0.053608	4.815560
257.102457	8000.222789	12.118746	-0.053637	4.815567
257.066654	8000.201927	12.123751	-0.053630	4.815562
257.102892	8000.212157	12.128755	-0.053637	4.815564
257.148531	8000.238565	12.133760	-0.053646	4.815572
257.036464	8000.210042	12.138765	-0.053625	4.815564
257.088735	8000.235491	12.143770	-0.053635	4.815571
257.080659	8000.211879	12.148775	-0.053634	4.815564
257.152427	8000.220555	12.153779	-0.053648	4.815567
257.304384	8000.215592	12.158784	-0.053676	4.815564
256.923086	8000.192268	12.163789	-0.053605	4.815559
257.208085	8000.230079	12.168794	-0.053659	4.815569
257.274378	8000.193800	12.173799	-0.053671	4.815558
257.291676	8000.203719	12.178803	-0.053675	4.815561
257.147032	8000.231279	12.183808	-0.053648	4.815570
257.191211	8000.210661	12.188813	-0.053657	4.815563
257.170291	8000.241318	12.193818	-0.053653	4.815572
257.113295	8000.242542	12.198823	-0.053643	4.815573
257.221701	8000.225113	12.203827	-0.053663	4.815567
257.379945	8000.227730	12.208832	-0.053693	4.815567
257.479400	8000.222974	12.213837	-0.053711	4.815566
257.510002	8000.234180	12.218842	-0.053717	4.815569
257.565142	8000.240448	12.223847	-0.053728	4.815570
257.221732	8000.215608	12.228851	-0.053664	4.815565
257.288834	8000.232754	12.233856	-0.053677	4.815569
257.278306	8000.220852	12.238861	-0.053675	4.815566
257.262937	8000.222758	12.243866	-0.053673	4.815567
257.218963	8000.230604	12.248871	-0.053665	4.815569
257.277379	8000.251881	12.253875	-0.053676	4.815575
257.402817	8000.233663	12.258880	-0.053699	4.815569
257.046682	8000.221434	12.263885	-0.053633	4.815567
257.120569	8000.238691	12.268890	-0.053647	4.815572
257.140849	8000.257206	12.273895	-0.053651	4.815577
257.337670	8000.233750	12.278899	-0.053688	4.815569
257.407934	8000.253084	12.283904	-0.053702	4.815575
257.288955	8000.215902	12.288909	-0.053680	4.815564
257.544742	8000.276737	12.293914	-0.053728	4.815581
257.374792	8000.251537	12.298919	-0.053696	4.815574
257.313772	8000.212101	12.303923	-0.053685	4.815563
257.266528	8000.248737	12.308928	-0.053676	4.815574
257.226885	8000.202173	12.313933	-0.053669	4.815561
257.232327	8000.238605	12.318938	-0.053671	4.815571
257.233468	8000.208734	12.323943	-0.053671	4.815562
257.220722	8000.194659	12.328947	-0.053669	4.815558
257.328294	8000.221015	12.333952	-0.053689	4.815566
257.198934	8000.185799	12.338957	-0.053665	4.815556
257.257331	8000.227372	12.343962	-0.053676	4.815568
257.089170	8000.237455	12.348967	-0.053645	4.815572
257.275471	8000.240532	12.353971	-0.053680	4.815572
257.364330	8000.246285	12.358976	-0.053697	4.815573
257.072270	8000.206263	12.363981	-0.053643	4.815562
257.297750	8000.250577	12.368986	-0.053685	4.815574
257.404768	8000.225648	12.373991	-0.053705	4.815567
257.109054	8000.226160	12.378995	-0.053651	4.815568
257.208827	8000.250252	12.384000	-0.053669	4.815575
257.382115	8000.228546	12.389005	-0.053702	4.815567
257.483887	8000.235578	12.394010	-0.053721	4.815569
257.204692	8000.224611	12.399015	-0.053669	4.815567
257.203409	8000.236362	12.404019	-0.053669	4.815571
257.512053	8000.247856	12.409024	-0.053727	4.815572
257.392531	8000.216006	12.414029	-0.053705	4.815564
257.481088	8000.233504	12.419034	-0.053722	4.815568
257.525402	8000.241731	12.424039	-0.053730	4.815571
257.236859	8000.244497	12.429043	-0.053677	4.815573
257.316640	8000.254373	12.434048	-0.053692	4.815575
257.210004	8000.208847	12.439053	-0.053672	4.815562
257.363776	8000.216733	12.444058	-0.053701	4.815564
257.329765	8000.215128	12.449063	-0.053695	4.815564
257.398502	8000.229096	12.454067	-0.053708	4.815567
257.224600	8000.232675	12.459072	-0.053676	4.815569
257.031204	8000.214569	12.464077	-0.053640	4.815565
257.129716	8000.239708	12.469082	-0.053659	4.815572
257.088733	8000.209146	12.474087	-0.053651	4.815563
257.213056	8000.210139	12.479091	-0.053675	4.815563
257.244638	8000.225634	12.484096	-0.053681	4.815567
257.007550	8000.198266	12.489101	-0.053637	4.815560
257.235612	8000.223393	12.494106	-0.053680	4.815567
257.191792	8000.224832	12.499111	-0.053672	4.815567
257.076605	8000.197327	12.504115	-0.053651	4.815560
257.275604	8000.225182	12.509120	-0.053688	4.815567
257.164892	8000.198818	12.514125	-0.053668	4.815560
257.145908	8000.230576	12.519130	-0.053664	4.815569
257.182153	8000.186326	12.524135	-0.053671	4.815556
257.275882	8000.215659	12.529139	-0.053689	4.815564
257.296648	8000.229909	12.534144	-0.053693	4.815568
257.236373	8000.224669	12.539149	-0.053682	4.815567
257.360060	8000.227788	12.544154	-0.053705	4.815567
257.306263	8000.227995	12.549159	-0.053696	4.815567
257.353571	8000.204223	12.554163	-0.053705	4.815560
257.573411	8000.228148	12.559168	-0.053746	4.815566
257.537548	8000.209421	12.564173	-0.053739	4.815561
257.443801	8000.223928	12.569178	-0.053722	4.815566
257.547765	8000.218178	12.574183	-0.053742	4.815563
257.392082	8000.218850	12.579187	-0.053713	4.815564
257.355870	8000.217210	12.584192	-0.053707	4.815564
257.189472	8000.195273	12.589197	-0.053676	4.815558
257.337477	8000.219088	12.594202	-0.053704	4.815565
257.502663	8000.229297	12.599207	-0.053735	4.815567
257.448563	8000.226295	12.604211	-0.053725	4.815566
257.619396	8000.239802	12.609216	-0.053757	4.815569
257.733323	8000.217122	12.614221	-0.053778	4.815562
257.617432	8000.263315	12.619226	-0.053757	4.815576
257.604214	8000.249232	12.624231	-0.053755	4.815572
257.405882	8000.241727	12.629235	-0.053718	4.815571
257.517862	8000.266019	12.634240	-0.053739	4.815577
257.443602	8000.222092	12.639245	-0.053726	4.815565
257.493818	8000.235757	12.644250	-0.053735	4.815569
257.435156	8000.233748	12.649255	-0.053725	4.815568
257.326985	8000.207425	12.654259	-0.053705	4.815561
257.330837	8000.226738	12.659264	-0.053706	4.815567
257.366876	8000.226283	12.664269	-0.053713	4.815567
257.272092	8000.230091	12.669274	-0.053695	4.815568
257.447679	8000.225515	12.674279	-0.053728	4.815566
257.467742	8000.223730	12.679283	-0.053732	4.815565
257.400570	8000.227991	12.684288	-0.053720	4.815567
257.224074	8000.201615	12.689293	-0.053687	4.815560
257.375485	8000.240442	12.694298	-0.053716	4.815571
257.415787	8000.219759	12.699303	-0.053723	4.815564
257.258782	8000.178748	12.704307	-0.053694	4.815553
257.393449	8000.210890	12.709312	-0.053720	4.815562
257.467152	8000.205711	12.714317	-0.053734	4.815560
257.455207	8000.239721	12.719322	-0.053732	4.815570
257.420859	8000.207132	12.724327	-0.053726	4.815561
257.502500	8000.224516	12.729331	-0.053741	4.815565
257.441858	8000.234226	12.734336	-0.053730	4.815568
257.222044	8000.203935	12.739341	-0.053689	4.815561
257.358781	8000.243589	12.744346	-0.053715	4.815572
257.497796	8000.230936	12.749351	-0.053741	4.815567
257.328430	8000.203609	12.754355	-0.053710	4.815560
257.254514	8000.233397	12.759360	-0.053696	4.815569
257.290700	8000.228671	12.764365	-0.053703	4.815567
257.460115	8000.243223	12.769370	-0.053735	4.815571
257.426591	8000.222398	12.774375	-0.053729	4.815565
257.581968	8000.213218	12.779379	-0.053758	4.815562
257.458764	8000.245403	12.784384	-0.053736	4.815572
257.350721	8000.197717	12.789389	-0.053716	4.815558
257.565461	8000.219422	12.794394	-0.053756	4.815563
257.520784	8000.226188	12.799399	-0.053748	4.815566
257.375265	8000.241983	12.804403	-0.053721	4.815571
257.565955	8000.233382	12.809408	-0.053757	4.815567
257.363596	8000.223674	12.814413	-0.053719	4.815566
257.582845	8000.244385	12.819418	-0.053760	4.815571
257.508577	8000.217550	12.824423	-0.053747	4.815563
257.279737	8000.243729	12.829427	-0.053704	4.815572
257.564811	8000.222789	12.834432	-0.053758	4.815564
257.462471	8000.192289	12.839437	-0.053739	4.815556
257.354028	8000.206555	12.844442	-0.053719	4.815561
257.463172	8000.203026	12.849447	-0.053740	4.815559
257.459875	8000.206199	12.854451	-0.053739	4.815560
257.676482	8000.263187	12.859456	-0.053780	4.815576
257.455965	8000.224338	12.864461	-0.053739	4.815565
257.441624	8000.239080	12.869466	-0.053737	4.815570
257.423840	8000.219581	12.874471	-0.053734	4.815564
257.437455	8000.211280	12.879475	-0.053736	4.815562
257.717784	8000.243676	12.884480	-0.053789	4.815570
257.356047	8000.200374	12.889485	-0.053722	4.815559
257.213806	8000.245066	12.894490	-0.053695	4.815572
257.472919	8000.231178	12.899495	-0.053744	4.815567
257.184256	8000.200826	12.904499	-0.053690	4.815560
257.389935	8000.221313	12.909504	-0.053729	4.815565
257.297128	8000.214471	12.914509	-0.053712	4.815563
257.598571	8000.232257	12.919514	-0.053768	4.815567
257.522679	8000.235307	12.924519	-0.053754	4.815568
257.373061	8000.171983	12.929523	-0.053727	4.815550
257.631767	8000.237140	12.934528	-0.053775	4.815568
257.615237	8000.203774	12.939533	-0.053772	4.815558
257.697836	8000.231858	12.944538	-0.053788	4.815566
257.710257	8000.227810	12.949543	-0.053791	4.815565
257.463951	8000.206699	12.954547	-0.053745	4.815560
257.492333	8000.238166	12.959552	-0.053750	4.815569
257.491338	8000.212533	12.964557	-0.053751	4.815562
257.520301	8000.235463	12.969562	-0.053756	4.815568
257.279140	8000.233665	12.974567	-0.053712	4.815569
257.306677	8000.222387	12.979571	-0.053717	4.815565
257.610722	8000.230602	12.984576	-0.053774	4.815566
257.348532	8000.188933	12.989581	-0.053725	4.815555
257.209297	8000.220855	12.994586	-0.053699	4.815565
257.353619	8000.218971	12.999591	-0.053727	4.815564
257.499352	8000.233135	13.004595	-0.053754	4.815567
257.501209	8000.246006	13.009600	-0.053755	4.815571
257.509259	8000.188473	13.014605	-0.053756	4.815554
257.591431	8000.226164	13.019610	-0.053772	4.815565
257.669864	8000.254179	13.024615	-0.053787	4.815573
257.500700	8000.236470	13.029619	-0.053755	4.815568
257.713101	8000.237840	13.034624	-0.053795	4.815568
257.647291	8000.234645	13.039629	-0.053783	4.815567
257.770195	8000.236683	13.044634	-0.053806	4.815567
257.833072	8000.240942	13.049639	-0.053818	4.815568
257.646490	8000.229356	13.054643	-0.053784	4.815566
257.549390	8000.243808	13.059648	-0.053766	4.815570
257.699816	8000.219591	13.064653	-0.053794	4.815562
257.858390	8000.225420	13.069658	-0.053824	4.815563
257.724940	8000.228593	13.074663	-0.053799	4.815565
257.665069	8000.197721	13.079667	-0.053789	4.815556
257.784586	8000.246707	13.084672	-0.053811	4.815570
257.784519	8000.217885	13.089677	-0.053811	4.815562
257.638038	8000.246483	13.094682	-0.053784	4.815571
257.780830	8000.262735	13.099687	-0.053811	4.815575
257.720469	8000.237196	13.104691	-0.053800	4.815567
257.647361	8000.238154	13.109696	-0.053787	4.815568
257.567161	8000.199471	13.114701	-0.053772	4.815557
257.745337	8000.233396	13.119706	-0.053805	4.815566
257.802518	8000.248243	13.124711	-0.053816	4.815570
257.486906	8000.215312	13.129715	-0.053758	4.815562
257.742138	8000.247296	13.134720	-0.053806	4.815570
257.794113	8000.244965	13.139725	-0.053816	4.815569
257.760353	8000.261526	13.144730	-0.053809	4.815574
257.682829	8000.244251	13.149735	-0.053795	4.815570
257.591728	8000.213935	13.154739	-0.053779	4.815561
257.627745	8000.242322	13.159744	-0.053786	4.815569
257.523605	8000.217134	13.164749	-0.053766	4.815562
257.719427	8000.224641	13.169754	-0.053803	4.815564
257.816079	8000.227317	13.174759	-0.053821	4.815564
257.617361	8000.232624	13.179763	-0.053785	4.815567
257.721849	8000.294184	13.184768	-0.053804	4.815584
257.675863	8000.256061	13.189773	-0.053796	4.815573
257.635467	8000.237259	13.194778	-0.053789	4.815568
257.598118	8000.246283	13.199783	-0.053782	4.815571
257.845551	8000.231135	13.204787	-0.053828	4.815565
257.789988	8000.249474	13.209792	-0.053818	4.815571
257.544299	8000.194188	13.214797	-0.053773	4.815556
257.562009	8000.236163	13.219802	-0.053776	4.815568
257.781957	8000.229110	13.224807	-0.053817	4.815565
257.502172	8000.229883	13.229811	-0.053766	4.815566
257.603307	8000.276431	13.234816	-0.053785	4.815579
257.675947	8000.253074	13.239821	-0.053798	4.815572
257.501544	8000.257712	13.244826	-0.053766	4.815574
257.524500	8000.252769	13.249831	-0.053771	4.815573
257.436280	8000.244934	13.254835	-0.053755	4.815571
257.521656	8000.273063	13.259840	-0.053771	4.815579
257.451029	8000.223854	13.264845	-0.053758	4.815565
257.472971	8000.246669	13.269850	-0.053762	4.815571
257.622874	8000.259833	13.274855	-0.053790	4.815574
257.566637	8000.246113	13.279859	-0.053780	4.815571
257.571839	8000.261176	13.284864	-0.053781	4.815575
257.657682	8000.230558	13.289869	-0.053797	4.815566
257.814687	8000.242770	13.294874	-0.053827	4.815568
257.665332	8000.239273	13.299879	-0.053799	4.815568
257.610918	8000.243743	13.304883	-0.053790	4.815570
257.695526	8000.266518	13.309888	-0.053806	4.815576
257.687510	8000.233292	13.314893	-0.053804	4.815566
257.671691	8000.236259	13.319898	-0.053802	4.815567
257.642617	8000.216575	13.324903	-0.053796	4.815562
257.474235	8000.222380	13.329907	-0.053765	4.815564
257.667467	8000.258688	13.334912	-0.053802	4.815574
257.788650	8000.228650	13.339917	-0.053824	4.815564
257.655218	8000.256394	13.344922	-0.053800	4.815573
257.775754	8000.239165	13.349927	-0.053822	4.815567
257.673201	8000.232162	13.354931	-0.053804	4.815566
257.713821	8000.255284	13.359936	-0.053811	4.815572
257.570236	8000.227312	13.364941	-0.053785	4.815565
257.624153	8000.238901	13.369946	-0.053795	4.815568
257.878394	8000.254845	13.374951	-0.053843	4.815572
257.643034	8000.227503	13.379955	-0.053799	4.815565
257.851587	8000.250175	13.384960	-0.053838	4.815570
257.812794	8000.200420	13.389965	-0.053831	4.815556
257.523188	8000.214919	13.394970	-0.053778	4.815562
257.585264	8000.238393	13.399975	-0.053789	4.815568
257.725297	8000.211869	13.404979	-0.053816	4.815560
257.703408	8000.235033	13.409984	-0.053812	4.815567
257.656729	8000.230016	13.414989	-0.053803	4.815565
257.584063	8000.239528	13.419994	-0.053790	4.815568
257.719018	8000.249242	13.424999	-0.053816	4.815571
257.561983	8000.231731	13.430003	-0.053787	4.815566
257.714281	8000.264163	13.435008	-0.053815	4.815575
257.735137	8000.237820	13.440013	-0.053819	4.815567
257.837769	8000.245936	13.445018	-0.053839	4.815569
257.774414	8000.259874	13.450023	-0.053827	4.815573
257.630624	8000.230829	13.455027	-0.053801	4.815566
257.691438	8000.247873	13.460032	-0.053812	4.815570
257.508730	8000.207507	13.465037	-0.053778	4.815559
257.591307	8000.249478	13.470042	-0.053794	4.815571
257.964784	8000.240672	13.475047	-0.053864	4.815567
257.610397	8000.230606	13.480051	-0.053798	4.815566
257.672211	8000.261553	13.485056	-0.053810	4.815574
257.720506	8000.224978	13.490061	-0.053819	4.815563
257.661912	8000.256086	13.495066	-0.053808	4.815573
257.587270	8000.238859	13.500071	-0.053795	4.815568
257.534420	8000.230536	13.505075	-0.053785	4.815566
257.728778	8000.244429	13.510080	-0.053822	4.815569
257.632340	8000.226844	13.515085	-0.053804	4.815564
257.781438	8000.237859	13.520090	-0.053832	4.815567
257.819128	8000.252386	13.525095	-0.053839	4.815571
257.898616	8000.240893	13.530099	-0.053854	4.815567
257.979745	8000.255065	13.535104	-0.053870	4.815571
257.976740	8000.242218	13.540109	-0.053869	4.815567
258.134329	8000.259782	13.545114	-0.053899	4.815572
257.838327	8000.230376	13.550119	-0.053844	4.815564
257.952022	8000.214103	13.555123	-0.053865	4.815559
257.744255	8000.252378	13.560128	-0.053827	4.815571
257.714548	8000.218795	13.565133	-0.053822	4.815562
257.815690	8000.240774	13.570138	-0.053841	4.815567
257.865812	8000.243755	13.575143	-0.053850	4.815568
257.862620	8000.239451	13.580147	-0.053850	4.815567
257.852299	8000.251054	13.585152	-0.053848	4.815570
257.932997	8000.208601	13.590157	-0.053863	4.815557
258.139158	8000.233371	13.595162	-0.053902	4.815564
258.075987	8000.247312	13.600167	-0.053891	4.815568
257.797036	8000.196820	13.605171	-0.053839	4.815555
258.201425	8000.248346	13.610176	-0.053914	4.815568
257.976316	8000.241468	13.615181	-0.053873	4.815567
257.732446	8000.250307	13.620186	-0.053828	4.815571
257.949566	8000.228253	13.625191	-0.053868	4.815563
258.179162	8000.234179	13.630195	-0.053911	4.815564
258.059114	8000.263211	13.635200	-0.053889	4.815573
257.899751	8000.222159	13.640205	-0.053860	4.815562
257.742024	8000.252709	13.645210	-0.053831	4.815571
257.777319	8000.247969	13.650215	-0.053837	4.815570
257.769366	8000.248928	13.655219	-0.053836	4.815570
257.789740	8000.255694	13.660224	-0.053840	4.815572
257.638019	8000.201949	13.665229	-0.053812	4.815557
257.662701	8000.235492	13.670234	-0.053817	4.815567
257.776347	8000.240583	13.675239	-0.053839	4.815567
257.662256	8000.221641	13.680243	-0.053818	4.815562
257.564808	8000.260658	13.685248	-0.053800	4.815574
257.780232	8000.214005	13.690253	-0.053840	4.815560
257.820691	8000.230715	13.695258	-0.053848	4.815564
257.847139	8000.246127	13.700263	-0.053853	4.815569
257.767617	8000.230956	13.705267	-0.053838	4.815565
257.942709	8000.240260	13.710272	-0.053871	4.815567
257.949502	8000.205140	13.715277	-0.053873	4.815556
257.851021	8000.239867	13.720282	-0.053855	4.815567
257.949783	8000.215871	13.725287	-0.053873	4.815559
257.763344	8000.238472	13.730291	-0.053839	4.815567
257.758161	8000.249091	13.735296	-0.053838	4.815570
257.731586	8000.218765	13.740301	-0.053833	4.815561
257.683732	8000.235094	13.745306	-0.053825	4.815566
257.802648	8000.231726	13.750311	-0.053847	4.815565
257.700132	8000.206563	13.755315	-0.053828	4.815558
257.867485	8000.256335	13.760320	-0.053860	4.815572
257.816263	8000.209580	13.765325	-0.053850	4.815558
257.757459	8000.225729	13.770330	-0.053840	4.815563
257.945747	8000.222431	13.775335	-0.053875	4.815561
257.861917	8000.202917	13.780339	-0.053860	4.815556
257.941219	8000.244834	13.785344	-0.053875	4.815568
257.849377	8000.231598	13.790349	-0.053858	4.815564
257.830785	8000.248407	13.795354	-0.053855	4.815569
257.880888	8000.226817	13.800359	-0.053864	4.815563
257.778399	8000.209132	13.805363	-0.053845	4.815558
258.040364	8000.256184	13.810368	-0.053894	4.815571
258.085617	8000.228105	13.815373	-0.053903	4.815562
257.934765	8000.240607	13.820378	-0.053875	4.815567
257.947508	8000.264340	13.825383	-0.053878	4.815573
257.899841	8000.234736	13.830387	-0.053869	4.815565
257.984154	8000.289555	13.835392	-0.053885	4.815581
257.772386	8000.235892	13.840397	-0.053846	4.815566
257.722066	8000.230815	13.845402	-0.053837	4.815565
257.733885	8000.219280	13.850407	-0.053839	4.815561
257.588272	8000.216912	13.855411	-0.053812	4.815561
257.793315	8000.247005	13.860416	-0.053851	4.815569
257.902301	8000.213562	13.865421	-0.053871	4.815559
257.649019	8000.231861	13.870426	-0.053824	4.815565
257.737205	8000.227989	13.875431	-0.053841	4.815564
257.714171	8000.181697	13.880435	-0.053837	4.815550
257.819363	8000.236858	13.885440	-0.053857	4.815566
257.663859	8000.231123	13.890445	-0.053828	4.815565
257.825134	8000.228450	13.895450	-0.053858	4.815563
257.996536	8000.236626	13.900455	-0.053891	4.815565
257.819846	8000.205973	13.905459	-0.053858	4.815557
257.949128	8000.279691	13.910464	-0.053882	4.815578
257.906989	8000.220266	13.915469	-0.053875	4.815561
257.734954	8000.221737	13.920474	-0.053843	4.815562
257.788961	8000.222645	13.925479	-0.053853	4.815562
257.885332	8000.208224	13.930483	-0.053871	4.815557
258.052094	8000.247304	13.935488	-0.053903	4.815568
257.762387	8000.223342	13.940493	-0.053849	4.815562
257.918505	8000.234472	13.945498	-0.053878	4.815565
258.151129	8000.228697	13.950503	-0.053922	4.815562
258.009349	8000.224255	13.955507	-0.053896	4.815561
257.981135	8000.257999	13.960512	-0.053891	4.815571
257.936342	8000.253012	13.965517	-0.053883	4.815570
257.912122	8000.238749	13.970522	-0.053878	4.815566
257.778181	8000.254733	13.975527	-0.053854	4.815571
257.927047	8000.234764	13.980531	-0.053882	4.815565
258.048739	8000.246397	13.985536	-0.053904	4.815567
257.711904	8000.221663	13.990541	-0.053842	4.815562
257.882049	8000.229818	13.995546	-0.053874	4.815563
257.968633	8000.249421	14.000551	-0.053890	4.815569
257.709457	8000.207800	14.005555	-0.053842	4.815558
257.758195	8000.254557	14.010560	-0.053852	4.815571
257.746428	8000.214859	14.015565	-0.053850	4.815560
257.765609	8000.248312	14.020570	-0.053854	4.815569
257.761653	8000.245064	14.025575	-0.053853	4.815568
257.868630	8000.246842	14.030579	-0.053873	4.815568
258.133746	8000.246941	14.035584	-0.053923	4.815567
258.003783	8000.211713	14.040589	-0.053899	4.815557
257.946158	8000.220404	14.045594	-0.053888	4.815560
257.795886	8000.269237	14.050599	-0.053861	4.815575
257.643237	8000.226159	14.055603	-0.053832	4.815563
257.786658	8000.264855	14.060608	-0.053859	4.815574
257.900520	8000.237902	14.065613	-0.053881	4.815566
257.804038	8000.218180	14.070618	-0.053863	4.815560
257.835160	8000.260375	14.075623	-0.053869	4.815572
258.106735	8000.226395	14.080627	-0.053920	4.815561
258.057889	8000.249118	14.085632	-0.053911	4.815568
257.906079	8000.235965	14.090637	-0.053883	4.815565
257.911142	8000.230729	14.095642	-0.053884	4.815563
258.092129	8000.255086	14.100647	-0.053918	4.815570
257.975621	8000.208328	14.105651	-0.053897	4.815557
257.958616	8000.288192	14.110656	-0.053894	4.815580
257.936011	8000.223745	14.115661	-0.053890	4.815561
258.049923	8000.235251	14.120666	-0.053911	4.815564
257.904853	8000.227551	14.125671	-0.053885	4.815562
257.846138	8000.210585	14.130675	-0.053874	4.815558
258.028899	8000.267020	14.135680	-0.053908	4.815573
257.963429	8000.248874	14.140685	-0.053896	4.815568
257.983874	8000.242822	14.145690	-0.053900	4.815567
257.992153	8000.247252	14.150695	-0.053902	4.815568
257.965529	8000.223335	14.155699	-0.053897	4.815561
257.838700	8000.251187	14.160704	-0.053874	4.815570
257.951642	8000.225287	14.165709	-0.053895	4.815562
257.856484	8000.216269	14.170714	-0.053878	4.815559
258.017175	8000.230679	14.175719	-0.053908	4.815563
257.974220	8000.232132	14.180723	-0.053900	4.815563
258.121948	8000.260217	14.185728	-0.053928	4.815571
258.030993	8000.225629	14.190733	-0.053911	4.815561
257.893471	8000.216984	14.195738	-0.053886	4.815559
258.175940	8000.259032	14.200743	-0.053939	4.815570
258.062190	8000.225138	14.205747	-0.053918	4.815561
258.178355	8000.266593	14.210752	-0.053940	4.815572
258.161158	8000.221464	14.215757	-0.053937	4.815559
258.260673	8000.251963	14.220762	-0.053956	4.815568
258.189605	8000.283935	14.225767	-0.053943	4.815577
257.982534	8000.228212	14.230771	-0.053904	4.815562
257.927465	8000.255106	14.235776	-0.053894	4.815570
257.883365	8000.217014	14.240781	-0.053886	4.815559
257.928236	8000.245547	14.245786	-0.053895	4.815567
258.020404	8000.271652	14.250791	-0.053912	4.815575
258.079149	8000.228838	14.255795	-0.053923	4.815562
258.000851	7999.287512	14.260800	-0.053908	4.815287

257.923704	7996.078717	14.265805	-0.053892	4.814350
258.002365	7990.584943	14.270810	-0.053904	4.812743
258.209287	7983.977615	14.275815	-0.053938	4.810810
257.927192	7976.614123	14.280819	-0.053881	4.808656
258.010858	7969.009192	14.285824	-0.053892	4.806430
257.812915	7961.173204	14.290829	-0.053850	4.804136
257.631172	7953.402006	14.295834	-0.053811	4.801859
257.738536	7945.388723	14.300839	-0.053826	4.799510
257.752629	7937.391777	14.305843	-0.053824	4.797164
257.642782	7929.386286	14.310848	-0.053799	4.794816
257.647600	7921.404505	14.315853	-0.053795	4.792472
257.657725	7913.343826	14.320858	-0.053792	4.790104
257.594490	7905.411427	14.325863	-0.053775	4.787774
257.350086	7897.346645	14.330867	-0.053724	4.785403
257.541662	7889.442611	14.335872	-0.053755	4.783077
257.546051	7881.404078	14.340877	-0.053751	4.780712
257.434586	7873.404024	14.345882	-0.053725	4.778356
257.416696	7865.435682	14.350887	-0.053717	4.776009
257.329471	7857.359185	14.355891	-0.053696	4.773629
257.440038	7849.388773	14.360896	-0.053711	4.771278
257.444450	7841.373317	14.365901	-0.053707	4.768913
257.274032	7833.390343	14.370906	-0.053670	4.766557
257.189271	7825.373329	14.375911	-0.053650	4.764190
257.043757	7817.400809	14.380915	-0.053618	4.761834
257.289288	7809.380950	14.385920	-0.053658	4.759463
257.159714	7801.397588	14.390925	-0.053629	4.757102
257.071120	7793.382853	14.395930	-0.053608	4.754730
256.788992	7785.309901	14.400935	-0.053550	4.752341
256.974888	7777.307392	14.405939	-0.053580	4.749970
257.010910	7769.332469	14.410944	-0.053582	4.747606
256.772702	7761.316494	14.415949	-0.053532	4.745230
256.917261	7753.334929	14.420954	-0.053554	4.742862
256.879229	7745.342815	14.425959	-0.053542	4.740490
256.573671	7737.377261	14.430963	-0.053480	4.738125
256.599806	7729.338188	14.435968	-0.053480	4.735736
256.962782	7721.326372	14.440973	-0.053543	4.733354
256.651418	7713.305781	14.445978	-0.053480	4.730969
256.330497	7705.313397	14.450983	-0.053415	4.728592
256.426743	7697.288063	14.455987	-0.053428	4.726202
256.521889	7689.322285	14.460992	-0.053441	4.723829
256.615345	7681.300770	14.465997	-0.053453	4.721438
256.428060	7673.278812	14.471002	-0.053414	4.719047
256.460167	7665.367447	14.476007	-0.053415	4.716686
256.206446	7657.299816	14.481011	-0.053362	4.714279
256.256972	7649.320343	14.486016	-0.053367	4.711896
256.052301	7641.295916	14.491021	-0.053324	4.709499
256.109385	7633.276588	14.496026	-0.053329	4.707102
256.089439	7625.274333	14.501031	-0.053321	4.704708
256.152349	7617.312221	14.506035	-0.053327	4.702326
256.213536	7609.288437	14.511040	-0.053334	4.699923
256.052435	7601.338095	14.516045	-0.053299	4.697542
256.306536	7593.280018	14.521050	-0.053341	4.695127
256.376371	7585.322671	14.526055	-0.053349	4.692740
256.002244	7577.269857	14.531059	-0.053275	4.690325
255.983959	7569.279621	14.536064	-0.053266	4.687927
255.945824	7561.264274	14.541069	-0.053254	4.685520
255.834478	7553.282783	14.546074	-0.053228	4.683122
255.716360	7545.357307	14.551079	-0.053202	4.680739
255.673510	7537.304523	14.556083	-0.053189	4.678317
255.844624	7529.303677	14.561088	-0.053215	4.675909
255.471836	7521.234822	14.566093	-0.053141	4.673480
255.410554	7513.148960	14.571098	-0.053125	4.671045
255.556630	7505.190459	14.576103	-0.053147	4.668646
255.386980	7497.220173	14.581107	-0.053110	4.666242
255.379450	7489.218516	14.586112	-0.053104	4.663828
255.601707	7481.261185	14.591117	-0.053140	4.661426
255.282309	7473.200495	14.596122	-0.053076	4.658992
255.482348	7465.274019	14.601127	-0.053108	4.656596
255.542495	7457.217926	14.606131	-0.053114	4.654160
255.536667	7449.216391	14.611136	-0.053108	4.651740
255.147207	7441.188020	14.616141	-0.053031	4.649310
255.190367	7433.232161	14.621146	-0.053034	4.646901
255.375198	7425.181876	14.626151	-0.053063	4.644462
255.045492	7417.251952	14.631155	-0.052997	4.642058
254.954454	7409.239301	14.636160	-0.052975	4.639628
254.964103	7401.284566	14.641165	-0.052972	4.637214
254.973255	7393.202393	14.646170	-0.052969	4.634760
255.029578	7385.175950	14.651175	-0.052974	4.632322
254.664353	7377.146998	14.656179	-0.052901	4.629882
254.833969	7369.177431	14.661184	-0.052928	4.627458
254.722385	7361.218899	14.666189	-0.052902	4.625037
254.628604	7353.181551	14.671194	-0.052880	4.622590
254.856362	7345.201966	14.676199	-0.052917	4.620159
254.760104	7337.198731	14.681203	-0.052894	4.617721
254.785444	7329.177269	14.686208	-0.052894	4.615275
254.735458	7321.202006	14.691213	-0.052880	4.612842
254.678607	7313.122588	14.696218	-0.052864	4.610376
254.522552	7305.175317	14.701223	-0.052830	4.607949
254.372054	7297.114828	14.706227	-0.052797	4.605486
254.481875	7289.177956	14.711232	-0.052813	4.603059
254.249946	7281.179251	14.716237	-0.052764	4.600613
254.102302	7273.171540	14.721242	-0.052732	4.598162
254.269627	7265.212576	14.726247	-0.052758	4.595725
254.256033	7257.124605	14.731251	-0.052751	4.593247
254.020339	7249.063808	14.736256	-0.052702	4.590776
254.151834	7241.102386	14.741261	-0.052721	4.588334
253.951956	7233.092986	14.746266	-0.052679	4.585876
253.946836	7225.173915	14.751271	-0.052673	4.583445
253.796305	7217.152744	14.756275	-0.052640	4.580980
254.008577	7209.106527	14.761280	-0.052675	4.578508
254.041554	7201.163557	14.766285	-0.052676	4.576065
253.789333	7193.109062	14.771290	-0.052624	4.573586
253.781861	7185.143387	14.776295	-0.052618	4.571134
253.734896	7177.106141	14.781299	-0.052604	4.568658
253.724630	7169.167325	14.786304	-0.052597	4.566212
253.667865	7161.130727	14.791309	-0.052582	4.563733
253.671544	7153.137730	14.796314	-0.052577	4.561267
253.544626	7145.114236	14.801319	-0.052549	4.558790
253.315448	7137.145134	14.806323	-0.052501	4.556329
253.356756	7129.112512	14.811328	-0.052504	4.553846
253.345264	7121.082500	14.816333	-0.052497	4.551363
253.106906	7113.094352	14.821338	-0.052447	4.548892
253.494705	7105.123483	14.826343	-0.052515	4.546425
253.544209	7097.077014	14.831347	-0.052519	4.543933
253.323090	7089.148277	14.836352	-0.052473	4.541476
253.136534	7081.112991	14.841357	-0.052433	4.538984
253.238823	7073.149875	14.846362	-0.052447	4.536514
253.211058	7065.128524	14.851367	-0.052437	4.534024
253.035766	7057.093451	14.856371	-0.052399	4.531528
253.046594	7049.108858	14.861376	-0.052396	4.529047
253.094444	7041.130400	14.866381	-0.052400	4.526567
252.810433	7033.049265	14.871386	-0.052342	4.524052
252.906145	7025.161539	14.876391	-0.052355	4.521597
252.901358	7017.087383	14.881395	-0.052349	4.519083
252.699199	7009.168477	14.886400	-0.052307	4.516615
252.756042	7001.120824	14.891405	-0.052312	4.514106
252.776413	6993.021891	14.896410	-0.052311	4.511580
252.746217	6985.043906	14.901415	-0.052301	4.509090
252.647430	6977.036941	14.906419	-0.052277	4.506589
252.630425	6969.047751	14.911424	-0.052269	4.504093
252.640817	6961.112682	14.916429	-0.052266	4.501612
252.520677	6953.046462	14.921434	-0.052239	4.499088
252.541593	6945.091234	14.926439	-0.052238	4.496599
252.634890	6937.055019	14.931443	-0.052250	4.494082
252.694298	6929.060455	14.936448	-0.052256	4.491578
252.467583	6921.039267	14.941453	-0.052209	4.489062
252.500710	6913.060890	14.946458	-0.052210	4.486560
252.408889	6905.062368	14.951463	-0.052188	4.484049
252.291913	6897.102419	14.956467	-0.052161	4.481549
252.254496	6889.046800	14.961472	-0.052149	4.479017
252.389911	6881.103114	14.966477	-0.052170	4.476520
252.344238	6872.996119	14.971482	-0.052156	4.473970
252.082578	6865.040942	14.976487	-0.052102	4.471465
252.019022	6856.990976	14.981491	-0.052086	4.468930
251.865788	6849.015974	14.986496	-0.052052	4.466416
251.674473	6841.000437	14.991501	-0.052012	4.463889
251.635006	6833.058958	14.996506	-0.051999	4.461383
251.933402	6825.010114	15.001511	-0.052050	4.458844
251.832695	6817.042771	15.006515	-0.052026	4.456327
251.744584	6808.994879	15.011520	-0.052005	4.453784
251.784618	6801.033914	15.016525	-0.052007	4.451267
251.780662	6792.984285	15.021530	-0.052002	4.448720
251.697175	6785.044824	15.026535	-0.051981	4.446206
251.666548	6777.002769	15.031539	-0.051970	4.443659
251.742760	6769.020050	15.036544	-0.051980	4.441130
251.523447	6761.054732	15.041549	-0.051934	4.438603
251.430668	6753.015568	15.046554	-0.051912	4.436052
251.561978	6745.009402	15.051559	-0.051931	4.433511
251.386700	6736.940396	15.056563	-0.051893	4.430947
251.308243	6728.970986	15.061568	-0.051874	4.428414
251.320651	6720.976389	15.066573	-0.051871	4.425872
251.167152	6712.980008	15.071578	-0.051838	4.423327
251.038470	6704.988907	15.076583	-0.051809	4.420782
251.063335	6696.998181	15.081587	-0.051808	4.418237
251.087703	6688.969960	15.086592	-0.051808	4.415678
251.093522	6680.986802	15.091597	-0.051804	4.413132
251.092268	6672.935991	15.096602	-0.051799	4.410563
251.083893	6665.003382	15.101607	-0.051792	4.408030
250.775390	6656.951223	15.106611	-0.051730	4.405456
250.818228	6648.997761	15.111616	-0.051733	4.402914
250.891362	6641.011302	15.116621	-0.051742	4.400359
250.544905	6633.016959	15.121626	-0.051672	4.397799
250.621230	6625.001759	15.126631	-0.051681	4.395233
250.779231	6616.945015	15.131635	-0.051706	4.392652
250.752862	6608.921447	15.136640	-0.051696	4.390080
250.549057	6600.986452	15.141645	-0.051653	4.387533
250.483265	6592.961340	15.146650	-0.051636	4.384957
250.614228	6585.039504	15.151655	-0.051655	4.382413
250.487731	6576.948164	15.156659	-0.051627	4.379812
250.407713	6569.005466	15.161664	-0.051607	4.377258
250.583834	6561.003548	15.166669	-0.051635	4.374684
250.559653	6552.953775	15.171674	-0.051625	4.372093
250.469788	6544.965258	15.176679	-0.051603	4.369519
250.106853	6536.985715	15.181683	-0.051531	4.366945
250.315738	6528.964238	15.186688	-0.051565	4.364359
250.263230	6521.051164	15.191693	-0.051550	4.361806
250.039382	6512.944085	15.196698	-0.051503	4.359187
250.085900	6505.039495	15.201703	-0.051507	4.356633
250.124414	6496.959143	15.206707	-0.051509	4.354021
250.118142	6488.844976	15.211712	-0.051503	4.351397
249.934706	6480.906149	15.216717	-0.051464	4.348826
249.663966	6472.888120	15.221722	-0.051409	4.346227
249.828917	6464.948788	15.226727	-0.051434	4.343656
249.651385	6456.954857	15.231731	-0.051396	4.341063
249.786049	6448.926470	15.236736	-0.051416	4.338459
249.794163	6440.983434	15.241741	-0.051413	4.335880
249.549527	6432.940071	15.246746	-0.051363	4.333266
249.780842	6424.924936	15.251751	-0.051401	4.330663
249.759057	6416.931600	15.256755	-0.051392	4.328063
249.578669	6408.930285	15.261760	-0.051353	4.325458
249.513377	6400.949515	15.266765	-0.051336	4.322859
249.382325	6392.931949	15.271770	-0.051307	4.320246
249.302785	6385.017693	15.276775	-0.051287	4.317665
249.276962	6376.920402	15.281779	-0.051277	4.315024
249.160160	6368.925809	15.286784	-0.051250	4.312413
249.201532	6360.904715	15.291789	-0.051253	4.309794
248.939228	6352.916627	15.296794	-0.051199	4.307181
249.005846	6344.942895	15.301799	-0.051207	4.304575
248.889372	6336.922063	15.306803	-0.051180	4.301949
248.809672	6328.911017	15.311808	-0.051160	4.299326
248.934127	6320.992363	15.316813	-0.051178	4.296733
248.888148	6312.905515	15.321818	-0.051165	4.294082
248.862486	6304.934518	15.326823	-0.051155	4.291467
248.668005	6296.872737	15.331827	-0.051114	4.288819
248.776835	6288.927226	15.336832	-0.051129	4.286211
248.912223	6280.908913	15.341837	-0.051149	4.283577
248.524154	6272.902140	15.346842	-0.051072	4.280941
248.598915	6264.959759	15.351847	-0.051081	4.278329
248.617103	6256.923174	15.356851	-0.051080	4.275683
248.587047	6248.905134	15.361856	-0.051069	4.273042
248.383058	6240.865380	15.366861	-0.051026	4.270390
248.360267	6232.867565	15.371866	-0.051017	4.267752
248.513556	6224.899350	15.376871	-0.051040	4.265123
248.092985	6216.852117	15.381875	-0.050957	4.262462
248.104818	6208.879656	15.386880	-0.050954	4.259828
248.279521	6200.908651	15.391885	-0.050982	4.257194
248.096279	6192.907024	15.396890	-0.050943	4.254545
248.284214	6184.875730	15.401895	-0.050973	4.251888
248.278277	6176.867954	15.406899	-0.050967	4.249235
248.227227	6168.882455	15.411904	-0.050952	4.246587
248.228692	6160.915542	15.416909	-0.050948	4.243945
248.280820	6152.905144	15.421914	-0.050952	4.241287
248.358702	6144.946950	15.426919	-0.050962	4.238645
247.894420	6136.940690	15.431923	-0.050871	4.235980
248.160286	6128.896981	15.436928	-0.050915	4.233308
248.042024	6120.885370	15.441933	-0.050888	4.230641
247.948353	6112.913767	15.446938	-0.050866	4.227986
248.104757	6104.908930	15.451943	-0.050890	4.225321
248.119609	6096.957291	15.456947	-0.050888	4.222670
247.899717	6088.865145	15.461952	-0.050842	4.219969
247.756099	6080.972344	15.466957	-0.050810	4.217333
247.739941	6072.905945	15.471962	-0.050802	4.214638
247.795995	6064.941508	15.476967	-0.050807	4.211977
247.358008	6056.907631	15.481971	-0.050721	4.209286
247.571924	6048.930794	15.486976	-0.050756	4.206619
247.640602	6040.929888	15.491981	-0.050764	4.203941
247.531327	6032.962901	15.496986	-0.050738	4.201270
247.539497	6024.951730	15.501991	-0.050735	4.198584
247.405953	6016.965052	15.506995	-0.050705	4.195903
247.329903	6008.854347	15.512000	-0.050686	4.193180
247.276061	6000.820707	15.517005	-0.050671	4.190480
247.284984	5992.833890	15.522010	-0.050668	4.187796
247.070848	5984.893752	15.527015	-0.050623	4.185123
246.875594	5976.925710	15.532019	-0.050581	4.182439
247.030628	5968.878186	15.537024	-0.050605	4.179730
247.052601	5960.950411	15.542029	-0.050604	4.177059
246.936600	5952.876799	15.547034	-0.050578	4.174335
246.759327	5944.891019	15.552039	-0.050540	4.171638
246.981400	5936.859193	15.557043	-0.050576	4.168928
246.962982	5928.854473	15.562048	-0.050568	4.166223
246.953283	5920.888824	15.567053	-0.050561	4.163530
246.831893	5912.910011	15.572058	-0.050534	4.160829
246.851063	5904.922394	15.577063	-0.050532	4.158125
246.685063	5896.934386	15.582067	-0.050496	4.155417
246.593573	5888.901199	15.587072	-0.050474	4.152693
246.577346	5880.839421	15.592077	-0.050466	4.149958
246.609256	5872.841965	15.597082	-0.050467	4.147244
246.428956	5864.882954	15.602087	-0.050429	4.144538
246.658290	5856.872449	15.607091	-0.050466	4.141818
246.486883	5848.857555	15.612096	-0.050430	4.139090
246.222317	5840.939398	15.617101	-0.050375	4.136392
246.114531	5832.868743	15.622106	-0.050350	4.133642
246.262611	5824.824457	15.627111	-0.050373	4.130903
246.334331	5816.875180	15.632115	-0.050381	4.128193
246.137619	5808.897035	15.637120	-0.050340	4.125468
246.261573	5800.927061	15.642125	-0.050358	4.122748
246.221082	5792.858785	15.647130	-0.050345	4.119991
246.072590	5784.951475	15.652135	-0.050313	4.117285
246.041160	5776.929204	15.657139	-0.050302	4.114540
246.116584	5768.819868	15.662144	-0.050311	4.111765
246.005345	5760.837818	15.667149	-0.050285	4.109029
245.761663	5752.866169	15.672154	-0.050235	4.106292
245.964349	5744.886534	15.677159	-0.050268	4.103558
245.881150	5736.894931	15.682163	-0.050247	4.100813
245.760543	5728.872006	15.687168	-0.050220	4.098055
245.756573	5720.923556	15.692173	-0.050214	4.095323
245.619757	5712.921177	15.697178	-0.050184	4.092568
245.690772	5704.888911	15.702183	-0.050192	4.089805
245.685667	5696.913070	15.707187	-0.050186	4.087057
245.686359	5688.882611	15.712192	-0.050181	4.084289
245.632512	5680.970160	15.717197	-0.050166	4.081559
245.393343	5672.906766	15.722202	-0.050117	4.078773
245.431175	5664.968897	15.727207	-0.050119	4.076032
245.400391	5656.911804	15.732211	-0.050108	4.073247
245.456677	5648.903637	15.737216	-0.050114	4.070478
245.431972	5640.928546	15.742221	-0.050104	4.067717
245.307542	5632.875554	15.747226	-0.050076	4.064927
245.229820	5624.950503	15.752231	-0.050056	4.062179
245.202818	5616.898274	15.757235	-0.050046	4.059386
245.242885	5608.950441	15.762240	-0.050049	4.056628
245.183585	5600.919580	15.767245	-0.050033	4.053838
245.129693	5592.900339	15.772250	-0.050018	4.051051
245.031485	5584.945049	15.777255	-0.049995	4.048283
245.019387	5576.938697	15.782259	-0.049987	4.045496
244.921981	5568.963898	15.787264	-0.049964	4.042718
244.865618	5560.969595	15.792269	-0.049949	4.039931
244.988744	5552.936457	15.797274	-0.049967	4.037132
244.925093	5544.928509	15.802279	-0.049950	4.034336
244.588999	5536.787778	15.807283	-0.049882	4.031488
244.605802	5528.832315	15.812288	-0.049881	4.028708
244.732951	5520.877531	15.817293	-0.049899	4.025929
244.620934	5512.893187	15.822298	-0.049873	4.023133
244.666200	5504.911983	15.827303	-0.049877	4.020339
244.725149	5496.921461	15.832307	-0.049883	4.017540
244.673207	5488.876444	15.837312	-0.049868	4.014718
244.528085	5480.889289	15.842317	-0.049836	4.011912
244.499188	5472.854595	15.847322	-0.049826	4.009090
244.335748	5464.936420	15.852327	-0.049791	4.006305
244.198158	5456.930362	15.857331	-0.049760	4.003488
244.237939	5448.952113	15.862336	-0.049762	4.000681
244.231064	5440.972717	15.867341	-0.049756	3.997871
244.041234	5432.907236	15.872346	-0.049716	3.995025
244.087422	5424.902235	15.877351	-0.049720	3.992203
244.033696	5416.857968	15.882355	-0.049705	3.989363
244.032425	5408.916886	15.887360	-0.049699	3.986559
243.989012	5400.912713	15.892365	-0.049686	3.983729
243.948984	5392.907034	15.897370	-0.049674	3.980897
243.815281	5384.958204	15.902375	-0.049644	3.978082
243.806730	5376.956300	15.907379	-0.049637	3.975248
243.656508	5368.906934	15.912384	-0.049605	3.972392
243.672183	5360.899544	15.917389	-0.049602	3.969552
243.553578	5352.896373	15.922394	-0.049575	3.966710
243.565556	5344.949857	15.927399	-0.049573	3.963888
243.559896	5336.952778	15.932403	-0.049567	3.961045
243.334148	5328.984351	15.937408	-0.049520	3.958207
243.438766	5320.969790	15.942413	-0.049534	3.955356
243.339826	5312.939330	15.947418	-0.049511	3.952494
243.247196	5304.924933	15.952423	-0.049489	3.949635
243.334304	5296.950439	15.957427	-0.049500	3.946792
243.253056	5288.954980	15.962432	-0.049480	3.943936
243.489038	5280.983747	15.967437	-0.049519	3.941093
243.238709	5272.972460	15.972442	-0.049467	3.938224
243.163048	5264.997679	15.977447	-0.049448	3.935370
243.327249	5256.973148	15.982451	-0.049474	3.932500
243.203889	5248.943582	15.987456	-0.049446	3.929620
243.201720	5240.989580	15.992461	-0.049440	3.926769
243.069260	5232.962715	15.997466	-0.049411	3.923886
243.138823	5224.978488	16.002471	-0.049419	3.921020
243.130034	5216.999726	16.007475	-0.049412	3.918153
243.042124	5208.983997	16.012480	-0.049391	3.915269
242.914223	5200.971936	16.017485	-0.049362	3.912383
242.741935	5192.931739	16.022490	-0.049325	3.909484
242.822921	5184.984928	16.027495	-0.049335	3.906622
242.672177	5177.002300	16.032499	-0.049302	3.903740
242.606532	5168.987480	16.037504	-0.049285	3.900846
242.618362	5161.016062	16.042509	-0.049282	3.897967
242.667377	5152.951886	16.047514	-0.049286	3.895053
242.696979	5144.977574	16.052519	-0.049287	3.892169
242.523424	5136.955257	16.057523	-0.049250	3.889261
242.383287	5128.995822	16.062528	-0.049218	3.886375
242.468009	5120.999396	16.067533	-0.049229	3.883477
242.416647	5113.005865	16.072538	-0.049215	3.880576
242.443657	5105.045934	16.077543	-0.049215	3.877686
242.318272	5097.018550	16.082547	-0.049187	3.874767
242.218215	5088.768489	16.087552	-0.049163	3.871765
241.949621	5080.833294	16.092557	-0.049108	3.868872
242.063392	5072.853345	16.097562	-0.049124	3.865968
242.292659	5064.921846	16.102567	-0.049162	3.863081
242.190463	5056.975855	16.107571	-0.049138	3.860181
241.954426	5048.968015	16.112576	-0.049089	3.857253
241.876908	5040.984947	16.117581	-0.049070	3.854335
241.750066	5032.969722	16.122586	-0.049041	3.851402
241.799005	5024.964536	16.127591	-0.049045	3.848475
241.809330	5016.951387	16.132595	-0.049042	3.845541
241.590076	5009.006607	16.137600	-0.048996	3.842625
241.609729	5001.015387	16.142605	-0.048995	3.839695
241.529988	4993.046072	16.147610	-0.048975	3.836769
241.643496	4985.043904	16.152615	-0.048991	3.833832
241.347264	4976.996364	16.157619	-0.048931	3.830868
241.368196	4968.999055	16.162624	-0.048930	3.827927
241.626820	4960.996002	16.167629	-0.048973	3.824987
241.369866	4953.043811	16.172634	-0.048921	3.822052
241.362474	4945.069943	16.177639	-0.048914	3.819112
241.249948	4937.133668	16.182643	-0.048888	3.816181
241.200701	4929.067189	16.187648	-0.048874	3.813201
241.149315	4921.073036	16.192653	-0.048860	3.810246
241.011640	4913.076645	16.197658	-0.048829	3.807286
240.954458	4905.061593	16.202663	-0.048813	3.804318
241.043477	4897.109961	16.207667	-0.048825	3.801375
240.884349	4889.097408	16.212672	-0.048790	3.798401
241.197797	4881.096930	16.217677	-0.048844	3.795440
240.883851	4873.035531	16.222682	-0.048780	3.792440
240.887180	4865.044931	16.227687	-0.048776	3.789471
240.740981	4857.066163	16.232691	-0.048744	3.786500
240.839120	4849.046395	16.237696	-0.048757	3.783518
240.745461	4841.086327	16.242701	-0.048735	3.780551
240.814633	4833.079208	16.247706	-0.048743	3.777568
240.903051	4825.067187	16.252711	-0.048754	3.774581
240.667538	4817.074430	16.257715	-0.048705	3.771592
240.319760	4809.068219	16.262720	-0.048636	3.768593
240.533296	4801.087700	16.267725	-0.048670	3.765613
240.442851	4793.092824	16.272730	-0.048649	3.762619
240.413960	4785.063914	16.277735	-0.048638	3.759611
240.315428	4777.119004	16.282739	-0.048615	3.756631
240.315112	4769.114481	16.287744	-0.048610	3.753628
240.323229	4761.080934	16.292749	-0.048606	3.750613
240.068215	4753.098453	16.297754	-0.048554	3.747607
240.297772	4745.083968	16.302759	-0.048592	3.744599
240.215765	4737.133467	16.307763	-0.048572	3.741605
240.026471	4729.109106	16.312768	-0.048531	3.738578
240.237371	4721.133197	16.317773	-0.048566	3.735577
240.119057	4713.106642	16.322778	-0.048539	3.732546
240.139402	4705.112596	16.327783	-0.048537	3.729528
239.925525	4697.143203	16.332787	-0.048493	3.726512
239.875895	4689.096451	16.337792	-0.048478	3.723467
239.963215	4681.166285	16.342797	-0.048490	3.720468
239.774169	4673.190996	16.347802	-0.048450	3.717443
240.080196	4665.162463	16.352807	-0.048502	3.714406
239.811348	4657.082858	16.357811	-0.048447	3.711334
239.637086	4649.082842	16.362816	-0.048409	3.708292
239.820134	4641.122948	16.367821	-0.048438	3.705272
239.486426	4633.161257	16.372826	-0.048371	3.702235
239.534806	4625.196065	16.377831	-0.048375	3.699204
239.599749	4617.199440	16.382835	-0.048382	3.696160
239.577368	4609.159460	16.387840	-0.048373	3.693093
239.470687	4601.177520	16.392845	-0.048348	3.690045
239.345947	4593.182995	16.397850	-0.048320	3.686988
239.386250	4585.182593	16.402855	-0.048323	3.683931
239.313248	4577.226530	16.407859	-0.048304	3.680886
239.145086	4569.235341	16.412864	-0.048268	3.677822
238.999876	4561.265645	16.417869	-0.048236	3.674764
239.181750	4553.192040	16.422874	-0.048265	3.671672
239.116024	4545.223102	16.427879	-0.048248	3.668612
239.080522	4537.211696	16.432883	-0.048236	3.665533
238.959586	4529.200642	16.437888	-0.048209	3.662450
239.002944	4521.233102	16.442893	-0.048212	3.659385
238.751697	4513.267134	16.447898	-0.048160	3.656311
238.795797	4505.244939	16.452903	-0.048163	3.653220
238.501541	4497.231622	16.457907	-0.048103	3.650120
238.436401	4489.222469	16.462912	-0.048086	3.647026
238.516587	4481.256991	16.467917	-0.048096	3.643950
238.493577	4473.254494	16.472922	-0.048087	3.640854
238.485426	4465.302936	16.477927	-0.048081	3.637776
238.365553	4457.265181	16.482931	-0.048053	3.634659
238.291786	4449.243247	16.487936	-0.048035	3.631546
238.449573	4441.224948	16.492941	-0.048059	3.628438
238.256737	4433.239575	16.497946	-0.048018	3.625331
238.296004	4425.258513	16.502951	-0.048020	3.622230
238.283315	4417.271084	16.507955	-0.048013	3.619121
238.408005	4409.315301	16.512960	-0.048031	3.616027
238.310320	4401.315545	16.517965	-0.048008	3.612906
238.158107	4393.265821	16.522970	-0.047975	3.609761
238.086947	4385.314930	16.527975	-0.047957	3.606655
237.899518	4377.319323	16.532979	-0.047917	3.603525
238.025915	4369.332258	16.537984	-0.047935	3.600405
237.957552	4361.375588	16.542989	-0.047918	3.597288
237.715044	4353.375443	16.547994	-0.047868	3.594147
237.841423	4345.348667	16.552999	-0.047886	3.591002
237.896483	4337.353898	16.558003	-0.047891	3.587866
237.770757	4329.349009	16.563008	-0.047863	3.584718
237.780954	4321.417534	16.568013	-0.047860	3.581600
237.986748	4313.351056	16.573018	-0.047893	3.578431
237.906025	4305.407626	16.578023	-0.047873	3.575300
237.785975	4297.398083	16.583027	-0.047846	3.572139
237.819507	4289.348828	16.588032	-0.047847	3.568964
237.769169	4281.421941	16.593037	-0.047833	3.565832
237.413956	4273.414015	16.598042	-0.047762	3.562656
237.339273	4265.421826	16.603047	-0.047743	3.559492
237.310184	4257.457042	16.608051	-0.047733	3.556337
237.139684	4249.362626	16.613056	-0.047696	3.553124
237.158483	4241.308698	16.618061	-0.047694	3.549930
237.079477	4233.361281	16.623066	-0.047675	3.546772
237.088210	4225.383783	16.628071	-0.047671	3.543602
237.245845	4217.386546	16.633075	-0.047696	3.540425
237.220183	4209.400821	16.638080	-0.047686	3.537245
237.177613	4201.410259	16.643085	-0.047673	3.534060
236.971260	4193.424461	16.648090	-0.047630	3.530869
237.182508	4185.431478	16.653095	-0.047664	3.527684
237.076665	4177.419770	16.658099	-0.047639	3.524480
236.801652	4169.492291	16.663104	-0.047583	3.521301
236.778654	4161.516184	16.668109	-0.047574	3.518107
236.755394	4153.495171	16.673114	-0.047565	3.514893
236.993330	4145.452094	16.678119	-0.047604	3.511675
236.793279	4137.439935	16.683123	-0.047562	3.508453
236.658946	4129.454234	16.688128	-0.047532	3.505240
236.817287	4121.502137	16.693133	-0.047556	3.502047
236.637411	4113.504408	16.698138	-0.047518	3.498822
236.436070	4105.553765	16.703143	-0.047476	3.495613
236.377978	4097.544398	16.708147	-0.047460	3.492381
236.490532	4089.500519	16.713152	-0.047476	3.489138
236.394871	4081.566140	16.718157	-0.047453	3.485930
236.352746	4073.583201	16.723162	-0.047440	3.482700
236.461275	4065.558811	16.728167	-0.047455	3.479456
236.423241	4057.619681	16.733171	-0.047443	3.476239
236.225370	4049.575916	16.738176	-0.047402	3.472970
236.194831	4041.568819	16.743181	-0.047391	3.469719
236.038977	4033.571537	16.748186	-0.047357	3.466465
236.046710	4025.580300	16.753191	-0.047353	3.463216
235.969767	4017.612536	16.758195	-0.047334	3.459970
235.877490	4009.624412	16.763200	-0.047312	3.456713
235.824862	4001.618489	16.768205	-0.047297	3.453446
235.675163	3993.598939	16.773210	-0.047264	3.450168
235.971923	3985.598387	16.778215	-0.047315	3.446909
235.821036	3977.641501	16.783219	-0.047282	3.443650
235.657809	3969.639862	16.788224	-0.047246	3.440369
235.657427	3961.684480	16.793229	-0.047241	3.437109
235.627688	3953.635567	16.798234	-0.047231	3.433807
235.556028	3945.640407	16.803239	-0.047212	3.430522
235.585427	3937.649221	16.808243	-0.047213	3.427240
235.372413	3929.658273	16.813248	-0.047168	3.423946
235.434984	3921.688061	16.818253	-0.047175	3.420666
235.251542	3913.735917	16.823258	-0.047136	3.417383
235.268501	3905.706098	16.828263	-0.047134	3.414071
235.454623	3897.683652	16.833267	-0.047164	3.410765
235.157785	3889.704489	16.838272	-0.047104	3.407457
235.136977	3881.723812	16.843277	-0.047095	3.404154
234.890925	3873.793049	16.848282	-0.047044	3.400862
234.980562	3865.784797	16.853287	-0.047056	3.397545
234.967742	3857.774866	16.858291	-0.047048	3.394221
234.855463	3849.663197	16.863296	-0.047022	3.390848
234.776612	3841.716708	16.868301	-0.047003	3.387541
234.661380	3833.722603	16.873306	-0.046976	3.384211
234.634975	3825.761870	16.878311	-0.046967	3.380893
234.678248	3817.803806	16.883315	-0.046970	3.377577
234.623842	3809.796804	16.888320	-0.046955	3.374233
234.718143	3801.795557	16.893325	-0.046967	3.370893
234.551878	3793.801317	16.898330	-0.046931	3.367544
234.468980	3785.820649	16.903335	-0.046911	3.364200
234.514827	3777.860745	16.908339	-0.046914	3.360866
234.395682	3769.847028	16.913344	-0.046887	3.357500
234.447256	3761.852709	16.918349	-0.046892	3.354145
234.158782	3753.841537	16.923354	-0.046833	3.350767
234.341981	3745.853385	16.928359	-0.046862	3.347413
234.390321	3737.839660	16.933363	-0.046866	3.344040
234.179410	3729.891326	16.938368	-0.046822	3.340681
234.463904	3721.892400	16.943373	-0.046870	3.337316
234.171936	3713.921461	16.948378	-0.046811	3.333938
234.233516	3705.904929	16.953383	-0.046817	3.330550
234.106208	3697.925625	16.958387	-0.046789	3.327168
234.110486	3689.933361	16.963392	-0.046785	3.323781
234.171613	3681.949385	16.968397	-0.046791	3.320397
233.942632	3673.999135	16.973402	-0.046743	3.317013
234.108591	3665.966374	16.978407	-0.046769	3.313605
233.958358	3657.927302	16.983411	-0.046736	3.310179
233.763696	3649.947464	16.988416	-0.046695	3.306773
233.686199	3641.995516	16.993421	-0.046676	3.303379
233.771581	3633.997764	16.998426	-0.046687	3.299969
233.528609	3626.047834	17.003431	-0.046636	3.296564
233.534614	3618.018990	17.008435	-0.046633	3.293130
233.562604	3610.003832	17.013440	-0.046633	3.289699
233.566996	3602.046475	17.018445	-0.046629	3.286289
233.360487	3594.060401	17.023450	-0.046585	3.282855
233.480620	3586.051803	17.028455	-0.046603	3.279420
233.327838	3578.119814	17.033459	-0.046569	3.276004
233.181811	3570.091885	17.038464	-0.046537	3.272543
233.301184	3562.083136	17.043469	-0.046554	3.269098
233.093953	3554.093747	17.048474	-0.046511	3.265644
233.050549	3546.124685	17.053479	-0.046498	3.262202
233.317972	3538.107441	17.058483	-0.046543	3.258747
233.205433	3530.122619	17.063488	-0.046517	3.255288
233.304480	3522.142736	17.068493	-0.046530	3.251836
233.074342	3514.141164	17.073498	-0.046482	3.248357
232.957569	3506.160815	17.078503	-0.046456	3.244888
232.860615	3498.206613	17.083507	-0.046433	3.241428
232.789284	3490.199756	17.088512	-0.046414	3.237943
232.769356	3482.214698	17.093517	-0.046406	3.234465
232.896311	3474.135806	17.098522	-0.046424	3.230948
232.855151	3466.176433	17.103527	-0.046412	3.227473
232.541938	3458.197525	17.108531	-0.046349	3.223974
232.677403	3450.194671	17.113536	-0.046369	3.220480
232.812821	3442.242492	17.118541	-0.046389	3.217004
232.346739	3434.286378	17.123546	-0.046297	3.213498
232.293241	3426.266860	17.128551	-0.046282	3.209977
232.478473	3418.274109	17.133555	-0.046312	3.206473
232.342348	3410.291331	17.138560	-0.046282	3.202957
232.375610	3402.326838	17.143565	-0.046283	3.199453
232.320144	3394.360376	17.148570	-0.046268	3.195939
232.311046	3386.335344	17.153575	-0.046261	3.192399
232.300321	3378.310901	17.158579	-0.046254	3.188854
232.214705	3370.320897	17.163584	-0.046233	3.185317
232.363004	3362.378722	17.168589	-0.046256	3.181808
232.224636	3354.362924	17.173594	-0.046225	3.178250
232.047955	3346.410497	17.178599	-0.046187	3.174714
232.183790	3338.398958	17.183603	-0.046207	3.171161
231.936900	3330.393301	17.188608	-0.046157	3.167591
231.824332	3322.439168	17.193613	-0.046131	3.164045
231.824130	3314.454407	17.198618	-0.046126	3.160487
231.782878	3306.491721	17.203623	-0.046113	3.156933
231.617738	3298.497696	17.208627	-0.046077	3.153355
231.439232	3290.452730	17.213632	-0.046039	3.149749
231.653012	3282.462356	17.218637	-0.046074	3.146182
231.625385	3274.461423	17.223642	-0.046064	3.142594
231.451637	3266.524313	17.228647	-0.046027	3.139025
231.514745	3258.557748	17.233651	-0.046033	3.135449
231.438618	3250.543888	17.238656	-0.046014	3.131842
231.606829	3242.541515	17.243661	-0.046041	3.128246
231.387413	3234.575525	17.248666	-0.045995	3.124646
231.184222	3226.637272	17.253671	-0.045952	3.121054
231.136141	3218.649351	17.258675	-0.045938	3.117443
231.113268	3210.615092	17.263680	-0.045929	3.113808
231.081862	3202.615882	17.268685	-0.045918	3.110184
230.886466	3194.628629	17.273690	-0.045877	3.106553
230.897340	3186.638420	17.278695	-0.045874	3.102927
230.981870	3178.674193	17.283699	-0.045885	3.099311
230.860367	3170.690541	17.288704	-0.045857	3.095673
230.895733	3162.693701	17.293709	-0.045859	3.092032
230.881891	3154.691386	17.298714	-0.045851	3.088382
230.985932	3146.692098	17.303719	-0.045865	3.084734
230.794040	3138.773810	17.308723	-0.045825	3.081105
230.636424	3130.808300	17.313728	-0.045790	3.077452
230.763076	3122.800975	17.318733	-0.045809	3.073789
230.600075	3114.704768	17.323738	-0.045774	3.070067
230.590861	3106.742703	17.328743	-0.045767	3.066409
230.383974	3098.797454	17.333747	-0.045724	3.062745
230.283489	3090.804169	17.338752	-0.045700	3.059060
230.301644	3082.859160	17.343757	-0.045698	3.055398
230.104558	3074.853177	17.348762	-0.045657	3.051694
230.237122	3066.840631	17.353767	-0.045676	3.047997
230.136519	3058.881347	17.358771	-0.045653	3.044310
230.110296	3050.913295	17.363776	-0.045643	3.040618
230.076821	3042.966452	17.368781	-0.045632	3.036930
230.005143	3034.953959	17.373786	-0.045613	3.033206
229.776123	3026.947565	17.378791	-0.045566	3.029472
229.820854	3018.962201	17.383795	-0.045569	3.025757
229.747544	3010.974168	17.388800	-0.045551	3.022031
229.856411	3002.995710	17.393805	-0.045566	3.018313
229.568014	2995.022545	17.398810	-0.045507	3.014573
229.685816	2987.013483	17.403815	-0.045524	3.010832
229.647927	2979.025347	17.408819	-0.045512	3.007088
229.446019	2971.057129	17.413824	-0.045470	3.003341
229.492139	2963.094063	17.418829	-0.045473	2.999604
229.407916	2955.125472	17.423834	-0.045453	2.995853
229.443320	2947.095256	17.428839	-0.045454	2.992075
229.210776	2939.130060	17.433843	-0.045406	2.988309
229.029236	2931.128621	17.438848	-0.045367	2.984523
229.165909	2923.169582	17.443853	-0.045388	2.980769
228.932774	2915.208500	17.448858	-0.045339	2.976991
228.849377	2907.213334	17.453863	-0.045319	2.973199
228.806429	2899.203694	17.458867	-0.045306	2.969397
228.962490	2891.214529	17.463872	-0.045330	2.965610
229.077412	2883.242530	17.468877	-0.045346	2.961825
228.878811	2875.272463	17.473882	-0.045305	2.958019
228.790720	2867.278599	17.478887	-0.045283	2.954203
228.822214	2859.280237	17.483891	-0.045284	2.950386
228.741748	2851.316068	17.488896	-0.045264	2.946575
228.767462	2843.329882	17.493901	-0.045264	2.942754
228.718763	2835.353672	17.498906	-0.045250	2.938928
228.756426	2827.381731	17.503911	-0.045252	2.935105
228.670799	2819.387495	17.508915	-0.045231	2.931259
228.556747	2811.378368	17.513920	-0.045205	2.927399
228.582899	2803.424111	17.518925	-0.045205	2.923568
228.438354	2795.466626	17.523930	-0.045173	2.919721
228.478073	2787.505946	17.528935	-0.045175	2.915878
228.370907	2779.445470	17.533939	-0.045150	2.911973
228.363407	2771.420315	17.538944	-0.045144	2.908086
228.489995	2763.453500	17.543949	-0.045163	2.904228
228.282378	2755.507148	17.548954	-0.045119	2.900358
228.173945	2747.561818	17.553959	-0.045094	2.896488
228.225718	2739.547896	17.558963	-0.045099	2.892589
228.193200	2731.552196	17.563968	-0.045088	2.888688
228.176820	2723.578935	17.568973	-0.045080	2.884794
228.106025	2715.643570	17.573978	-0.045062	2.880910
228.056228	2707.666896	17.578983	-0.045047	2.877002
228.031134	2699.676052	17.583987	-0.045038	2.873083
227.962621	2691.664766	17.588992	-0.045020	2.869146
227.912825	2683.695411	17.593997	-0.045006	2.865225
227.901715	2675.713630	17.599002	-0.044999	2.861295
227.899217	2667.748811	17.604007	-0.044993	2.857369
227.854239	2659.772558	17.609011	-0.044980	2.853429
227.745422	2651.764701	17.614016	-0.044955	2.849464
227.604167	2643.832851	17.619021	-0.044924	2.845530
227.666175	2635.858792	17.624026	-0.044930	2.841581
227.671096	2627.870215	17.629031	-0.044926	2.837615
227.437886	2619.915498	17.634035	-0.044878	2.833648
227.327510	2611.889113	17.639040	-0.044852	2.829646
227.529667	2603.896040	17.644045	-0.044885	2.825673
227.129813	2595.962937	17.649050	-0.044805	2.821690
227.081119	2587.985430	17.654055	-0.044791	2.817699
227.218637	2579.979814	17.659059	-0.044812	2.813699
227.110551	2572.002531	17.664064	-0.044787	2.809694
227.103336	2564.015748	17.669069	-0.044781	2.805684
226.946351	2556.071929	17.674074	-0.044747	2.801680
226.922365	2548.093825	17.679079	-0.044737	2.797662
226.933519	2540.120654	17.684083	-0.044734	2.793643
226.933684	2532.091029	17.689088	-0.044729	2.789588
226.796752	2524.159320	17.694093	-0.044699	2.785569
226.512525	2516.192191	17.699098	-0.044641	2.781518
226.765566	2508.182248	17.704103	-0.044683	2.777470
226.679295	2500.214824	17.709107	-0.044662	2.773419
226.517092	2492.220122	17.714112	-0.044627	2.769342
226.542329	2484.272907	17.719117	-0.044627	2.765296
226.641296	2476.278521	17.724122	-0.044640	2.761223
226.624494	2468.298475	17.729127	-0.044632	2.757145
226.445783	2460.334654	17.734131	-0.044594	2.753060
226.402410	2452.274268	17.739136	-0.044581	2.748927
226.329798	2444.341329	17.744141	-0.044562	2.744852
226.123884	2436.402583	17.749146	-0.044519	2.740759
225.995103	2428.454553	17.754151	-0.044490	2.736660
226.170658	2420.449732	17.759155	-0.044518	2.732544
225.836453	2412.465455	17.764160	-0.044451	2.728402
225.983176	2404.486952	17.769165	-0.044473	2.724285
225.907661	2396.545098	17.774170	-0.044454	2.720168
225.890122	2388.581321	17.779175	-0.044446	2.716037
225.742597	2380.584550	17.784179	-0.044413	2.711874
225.642445	2372.586071	17.789184	-0.044390	2.707707
225.930964	2364.597050	17.794189	-0.044439	2.703562
225.492366	2356.670398	17.799194	-0.044352	2.699398
225.442277	2348.717236	17.804199	-0.044338	2.695239
225.761952	2340.681754	17.809203	-0.044392	2.691053
225.683869	2332.710172	17.814208	-0.044373	2.686869
225.492665	2324.782549	17.819213	-0.044332	2.682694
225.479081	2316.811459	17.824218	-0.044325	2.678501
225.455782	2308.839227	17.829223	-0.044315	2.674300
225.130068	2300.861277	17.834227	-0.044250	2.670071
224.903964	2292.875178	17.839232	-0.044203	2.665836
225.291158	2284.882560	17.844237	-0.044270	2.661631
225.239917	2276.899365	17.849242	-0.044255	2.657396
225.018529	2268.957949	17.854247	-0.044209	2.653166
224.846798	2260.990687	17.859251	-0.044172	2.648918
224.672977	2253.014303	17.864256	-0.044135	2.644658
224.819996	2245.063791	17.869261	-0.044158	2.640426
224.796270	2237.078638	17.874266	-0.044148	2.636158
224.757974	2229.079373	17.879271	-0.044136	2.631874
224.753699	2221.113391	17.884275	-0.044130	2.627603
224.470745	2213.149491	17.889280	-0.044073	2.623308
224.435463	2205.209893	17.894285	-0.044061	2.619035
224.339703	2197.236337	17.899290	-0.044038	2.614733
224.480112	2189.220616	17.904295	-0.044060	2.610417
224.482884	2181.254515	17.909299	-0.044055	2.606112
224.675057	2173.269914	17.914304	-0.044086	2.601802
224.277022	2165.393338	17.919309	-0.044007	2.597503
224.334788	2157.314014	17.924314	-0.044013	2.593119
224.229580	2149.217978	17.929319	-0.043988	2.588706
224.276764	2141.280378	17.934323	-0.043992	2.584383
223.877937	2133.383160	17.939328	-0.043913	2.580044
223.988892	2125.436796	17.944333	-0.043928	2.575706
223.922888	2117.457415	17.949338	-0.043911	2.571330
223.822742	2109.501926	17.954343	-0.043888	2.566957
223.664752	2101.575864	17.959347	-0.043853	2.562590
223.664513	2093.594449	17.964352	-0.043848	2.558195
223.763071	2085.634587	17.969357	-0.043862	2.553811
223.690201	2077.633300	17.974362	-0.043843	2.549385
223.544870	2069.683331	17.979367	-0.043811	2.544975
223.557284	2061.731932	17.984371	-0.043809	2.540567
223.361323	2053.786339	17.989376	-0.043767	2.536140
223.598873	2045.778654	17.994381	-0.043806	2.531701
223.615434	2037.802758	17.999386	-0.043805	2.527257
223.395887	2029.874178	18.004391	-0.043759	2.522814
223.322669	2021.927544	18.009395	-0.043740	2.518364
223.522529	2013.917065	18.014400	-0.043772	2.513890
223.356391	2005.946393	18.019405	-0.043737	2.509404
223.094586	1997.987694	18.024410	-0.043683	2.504909
223.233912	1990.026848	18.029415	-0.043704	2.500435
223.068418	1982.096601	18.034419	-0.043668	2.495947
223.069239	1974.089406	18.039424	-0.043663	2.491420
222.962019	1966.149028	18.044429	-0.043638	2.486915
222.869968	1958.186226	18.049434	-0.043616	2.482390
223.011221	1950.221116	18.054439	-0.043638	2.477872
222.741712	1942.293226	18.059443	-0.043583	2.473337
222.693427	1934.296263	18.064448	-0.043569	2.468771
222.562557	1926.339086	18.069453	-0.043539	2.464212
222.689618	1918.371702	18.074458	-0.043558	2.459659
222.838917	1910.398404	18.079463	-0.043581	2.455096
222.660906	1902.436621	18.084467	-0.043543	2.450506
222.192174	1894.519095	18.089472	-0.043451	2.445911
222.306646	1886.563291	18.094477	-0.043467	2.441329
222.554067	1878.557354	18.099482	-0.043508	2.436720
222.484405	1870.575096	18.104487	-0.043490	2.432091
222.226089	1862.607991	18.109491	-0.043437	2.427448
222.075216	1854.646901	18.114496	-0.043404	2.422808
222.119129	1846.708279	18.119501	-0.043407	2.418188
221.852602	1838.766386	18.124506	-0.043353	2.413532
221.897314	1830.771698	18.129511	-0.043356	2.408860
221.901105	1822.813894	18.134515	-0.043352	2.404198
221.707960	1814.886859	18.139520	-0.043311	2.399530
221.905784	1806.926915	18.144525	-0.043343	2.394864
221.851236	1798.930333	18.149530	-0.043328	2.390147
221.710932	1790.989029	18.154535	-0.043297	2.385446
221.512015	1783.071840	18.159539	-0.043255	2.380746
221.469730	1775.104667	18.164544	-0.043242	2.376020
221.601150	1767.127135	18.169549	-0.043261	2.371291
221.282819	1759.188215	18.174554	-0.043197	2.366541
221.470905	1751.203723	18.179559	-0.043227	2.361794
221.408983	1743.285329	18.184563	-0.043211	2.357057
221.138114	1735.326748	18.189568	-0.043155	2.352269
221.300970	1727.327395	18.194573	-0.043181	2.347483
221.281747	1719.358024	18.199578	-0.043172	2.342689
220.885134	1711.479480	18.204583	-0.043094	2.337910
220.777920	1703.514940	18.209587	-0.043069	2.333093
220.854535	1695.522041	18.214592	-0.043078	2.328264
221.060505	1687.539862	18.219597	-0.043111	2.323442
220.774619	1679.635081	18.224602	-0.043053	2.318616
220.751942	1671.679709	18.229607	-0.043044	2.313771
220.742747	1663.719475	18.234611	-0.043037	2.308914
220.787109	1655.727323	18.239616	-0.043041	2.304032
220.683927	1647.823479	18.244621	-0.043017	2.299181
220.868479	1639.837897	18.249626	-0.043046	2.294294
220.659628	1631.892422	18.254631	-0.043002	2.289388
220.559807	1623.964000	18.259635	-0.042979	2.284491
220.443010	1616.027721	18.264640	-0.042952	2.279577
220.406297	1608.100572	18.269645	-0.042940	2.274665
220.260480	1600.057414	18.274650	-0.042908	2.269662
220.302529	1592.089775	18.279655	-0.042911	2.264710
220.261597	1584.177555	18.284659	-0.042898	2.259774
220.015360	1576.247269	18.289664	-0.042848	2.254799
220.066741	1568.278274	18.294669	-0.042852	2.249815
220.135292	1560.298652	18.299674	-0.042860	2.244814
219.827509	1552.415060	18.304679	-0.042798	2.239829
219.746061	1544.491607	18.309683	-0.042778	2.234828
219.800992	1536.488844	18.314688	-0.042783	2.229778
219.836185	1528.541402	18.319693	-0.042785	2.224749
219.681735	1520.622039	18.324698	-0.042751	2.219711
219.726372	1512.663599	18.329703	-0.042754	2.214653
219.852881	1504.696849	18.334707	-0.042773	2.209586
219.624792	1496.768708	18.339712	-0.042726	2.204500
219.520016	1488.863763	18.344717	-0.042701	2.199428
219.427015	1480.925164	18.349722	-0.042679	2.194324
219.414490	1472.928508	18.354727	-0.042672	2.189178
219.303487	1464.991194	18.359731	-0.042646	2.184050
218.914903	1457.101596	18.364736	-0.042569	2.178914
219.140348	1449.116918	18.369741	-0.042606	2.173761
219.002040	1441.181374	18.374746	-0.042575	2.168594
218.902753	1433.235078	18.379751	-0.042552	2.163412
218.981688	1425.305150	18.384755	-0.042562	2.158244
218.733825	1417.382902	18.389760	-0.042510	2.153039
218.735646	1409.419064	18.394765	-0.042506	2.147816
218.722881	1401.475950	18.399770	-0.042499	2.142594
218.725548	1393.547615	18.404775	-0.042494	2.137370
218.772423	1385.600904	18.409779	-0.042498	2.132125
218.535753	1377.669027	18.414784	-0.042449	2.126850
218.731026	1369.719448	18.419789	-0.042480	2.121591
218.489690	1361.825892	18.424794	-0.042431	2.116315
218.366780	1353.825023	18.429799	-0.042403	2.110965
218.509153	1345.854405	18.434803	-0.042424	2.105647
218.208927	1337.967163	18.439808	-0.042363	2.100329
218.239211	1330.030165	18.444813	-0.042364	2.094996
218.135123	1322.085879	18.449818	-0.042340	2.089632
218.071643	1314.156149	18.454823	-0.042323	2.084267
217.982869	1306.260205	18.459827	-0.042302	2.078909
217.776137	1298.338044	18.464832	-0.042258	2.073508
217.959684	1290.354993	18.469837	-0.042287	2.068090
217.997564	1282.410784	18.474842	-0.042290	2.062669
217.681401	1274.533732	18.479847	-0.042226	2.057245
217.629788	1266.604401	18.484851	-0.042211	2.051797
217.493473	1258.668250	18.489856	-0.042181	2.046321
217.476301	1250.749253	18.494861	-0.042173	2.040855
217.545622	1242.826803	18.499866	-0.042181	2.035380
217.392565	1234.861045	18.504871	-0.042147	2.029838
217.343590	1226.941676	18.509875	-0.042133	2.024323
217.117545	1219.035628	18.514880	-0.042086	2.018785
217.222985	1211.100645	18.519885	-0.042101	2.013245
217.125656	1203.163627	18.524890	-0.042078	2.007667
216.980713	1195.260204	18.529895	-0.042046	2.002093
217.033250	1187.342504	18.534899	-0.042051	1.996513
217.109574	1179.372597	18.539904	-0.042060	1.990884
216.926419	1171.473196	18.544909	-0.042021	1.985261
216.816790	1163.570003	18.549914	-0.041996	1.979627
216.654760	1155.675771	18.554919	-0.041961	1.973978
216.752036	1147.722810	18.559923	-0.041974	1.968298
216.389494	1139.847773	18.564928	-0.041902	1.962609
216.560537	1131.912043	18.569933	-0.041929	1.956916
216.471487	1123.952705	18.574938	-0.041907	1.951162
216.432253	1116.004458	18.579943	-0.041895	1.945404
216.190238	1108.132764	18.584947	-0.041845	1.939663
216.078948	1100.217781	18.589952	-0.041819	1.933887
216.184298	1092.278278	18.594957	-0.041834	1.928100
216.108236	1084.365609	18.599962	-0.041815	1.922295
215.862413	1076.489154	18.604967	-0.041764	1.916481
215.788138	1068.567475	18.609971	-0.041745	1.910634
215.556110	1060.656861	18.614976	-0.041697	1.904760
215.683869	1052.737268	18.619981	-0.041716	1.898901
215.863607	1044.794900	18.624986	-0.041745	1.893013
215.589143	1036.905376	18.629991	-0.041689	1.887095
215.620453	1029.004458	18.634995	-0.041690	1.881184
215.824692	1021.067705	18.640000	-0.041723	1.875248
215.587890	1013.173934	18.645005	-0.041674	1.869275
215.314552	1005.284543	18.650010	-0.041618	1.863281
215.364094	997.369080	18.655015	-0.041622	1.857286
215.299179	989.475316	18.660019	-0.041605	1.851274
215.291617	981.550012	18.665024	-0.041599	1.845226
215.227033	973.688932	18.670029	-0.041582	1.839200
215.072360	965.795662	18.675034	-0.041548	1.833118
214.785814	957.899845	18.680039	-0.041490	1.826999
214.983084	949.971037	18.685043	-0.041522	1.820892
214.604185	942.113741	18.690048	-0.041447	1.814750
214.641796	934.201373	18.695053	-0.041449	1.808595
214.475529	926.319874	18.700058	-0.041413	1.802418
214.462704	918.423841	18.705063	-0.041405	1.796227
214.620870	910.454585	18.710067	-0.041430	1.789978
214.342310	902.574858	18.715072	-0.041373	1.783724
214.358417	894.698803	18.720077	-0.041371	1.777487
214.437268	886.785479	18.725082	-0.041381	1.771207
214.150332	878.918629	18.730087	-0.041323	1.764895
214.136051	871.056862	18.735091	-0.041315	1.758600
214.066464	863.157966	18.740096	-0.041297	1.752244
214.051221	855.264365	18.745101	-0.041290	1.745877
213.773404	847.419468	18.750106	-0.041233	1.739493
213.865949	839.523264	18.755111	-0.041245	1.733090
213.880872	831.626243	18.760115	-0.041243	1.726653
213.717831	823.758400	18.765120	-0.041208	1.720193
213.578543	815.923495	18.770125	-0.041177	1.713739
213.624232	807.993626	18.775130	-0.041181	1.707206
213.512110	800.129069	18.780135	-0.041155	1.700681
213.526765	792.263660	18.785139	-0.041153	1.694147
213.195850	784.401926	18.790144	-0.041086	1.687545
213.411478	776.512416	18.795149	-0.041122	1.680967
213.222302	768.671727	18.800154	-0.041082	1.674349
213.294492	760.767715	18.805159	-0.041090	1.667687
213.521091	752.879991	18.810163	-0.041127	1.661033
213.057780	745.082620	18.815168	-0.041036	1.654336
213.175333	737.182416	18.820173	-0.041053	1.647602
213.119314	729.329288	18.825178	-0.041038	1.640858
212.943126	721.497606	18.830183	-0.041000	1.634088
212.964900	713.574291	18.835187	-0.040999	1.627237
212.937420	705.710960	18.840192	-0.040989	1.620403
213.088024	697.851515	18.845197	-0.041013	1.613568
212.695929	690.044096	18.850202	-0.040935	1.606673
212.556173	682.215492	18.855207	-0.040904	1.599766
212.573655	674.369405	18.860211	-0.040902	1.592835
212.478716	666.501937	18.865216	-0.040880	1.585839
212.403490	658.683682	18.870221	-0.040861	1.578859
212.492642	650.813818	18.875226	-0.040873	1.571826
212.431843	642.963920	18.880231	-0.040856	1.564756
212.340803	635.169025	18.885235	-0.040835	1.557700
211.978869	627.348661	18.890240	-0.040762	1.550549
212.074015	619.487864	18.895245	-0.040775	1.543396
212.069436	611.653495	18.900250	-0.040770	1.536218
211.974613	603.823961	18.905255	-0.040747	1.528998
211.998350	595.990923	18.910259	-0.040747	1.521758
211.774022	588.197068	18.915264	-0.040700	1.514482
211.606792	580.392162	18.920269	-0.040664	1.507170
211.554212	572.555732	18.925274	-0.040649	1.499810
211.650976	564.723087	18.930279	-0.040663	1.492440
211.571445	556.907153	18.935283	-0.040643	1.485022
211.258788	549.147037	18.940288	-0.040580	1.477583
211.396505	541.267978	18.945293	-0.040601	1.470064
211.403198	533.435422	18.950298	-0.040597	1.462530
211.155135	525.671465	18.955303	-0.040546	1.454983
211.382581	517.822323	18.960307	-0.040583	1.447389
211.218542	510.045023	18.965312	-0.040548	1.439763
210.995222	502.303745	18.970317	-0.040502	1.432122
210.883311	494.506265	18.975322	-0.040476	1.424403
210.847993	486.722897	18.980327	-0.040465	1.416668
210.894264	478.922624	18.985331	-0.040468	1.408887
210.686576	471.157573	18.990336	-0.040425	1.401056
210.658266	463.389211	18.995341	-0.040415	1.393208
210.646767	455.574671	19.000346	-0.040408	1.385271
210.395138	447.845030	19.005351	-0.040356	1.377334
210.405249	440.057633	19.010355	-0.040353	1.369337
210.186555	432.319513	19.015360	-0.040308	1.361304
210.288973	424.544155	19.020365	-0.040322	1.353241
210.076972	416.802475	19.025370	-0.040278	1.345109
209.974749	409.058702	19.030375	-0.040254	1.336945
210.087093	401.280581	19.035379	-0.040270	1.328733
210.004117	393.543296	19.040384	-0.040250	1.320478
210.020176	385.755561	19.045389	-0.040248	1.312135
209.731363	377.983623	19.050394	-0.040189	1.303700
209.513594	370.287913	19.055399	-0.040144	1.295306
209.636352	362.536078	19.060403	-0.040162	1.286858
209.606561	354.820323	19.065408	-0.040152	1.278366
209.375270	347.148388	19.070413	-0.040104	1.269828
209.297364	339.436931	19.075418	-0.040085	1.261218
209.094802	331.760477	19.080423	-0.040042	1.252563
209.163888	324.035892	19.085427	-0.040050	1.243846
209.028377	316.364290	19.090432	-0.040020	1.235088
208.863790	308.676401	19.095437	-0.039985	1.226243
208.983350	300.966012	19.100442	-0.040002	1.217364
208.844396	293.297390	19.105447	-0.039972	1.208417
208.917317	285.618855	19.110451	-0.039980	1.199434
208.778262	277.967823	19.115456	-0.039950	1.190373
208.510614	270.350123	19.120461	-0.039895	1.181256
208.693037	262.666034	19.125466	-0.039924	1.172080
208.399663	255.059327	19.130471	-0.039865	1.162828
208.238692	247.446155	19.135475	-0.039830	1.153521
207.938349	239.809643	19.140480	-0.039770	1.144080
208.192682	232.141819	19.145485	-0.039812	1.134639
208.057548	224.534597	19.150490	-0.039783	1.125111
207.776542	216.975739	19.155495	-0.039726	1.115532
207.706174	209.378625	19.160499	-0.039708	1.105867
207.439531	201.821889	19.165504	-0.039653	1.096125
207.234789	194.259175	19.170509	-0.039611	1.086301
207.002260	186.723943	19.175514	-0.039563	1.076418
207.018192	179.122372	19.180519	-0.039561	1.066412
206.930950	171.581853	19.185523	-0.039540	1.056369
206.764753	164.043535	19.190528	-0.039504	1.046214
206.779973	156.514271	19.195533	-0.039503	1.036014
206.688423	148.992151	19.200538	-0.039481	1.025697
206.439512	141.519087	19.205543	-0.039430	1.015306
206.495449	134.007229	19.210547	-0.039436	1.004827
206.329298	126.541656	19.215552	-0.039400	0.994249
206.285369	119.040259	19.220557	-0.039387	0.983535
205.948180	111.631448	19.225562	-0.039320	0.972764
206.156014	104.134820	19.230567	-0.039354	0.961883
206.039464	96.730754	19.235571	-0.039328	0.950930
205.599498	89.378333	19.240576	-0.039241	0.939843
205.415489	82.003706	19.245581	-0.039202	0.928657
205.313140	74.636733	19.250586	-0.039179	0.917368
204.837032	67.325770	19.255591	-0.039086	0.905924
204.944959	60.181050	19.260595	-0.039101	0.894757