Thu Mar 11 18:37:05 2021

Number of Points = 3619
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.511764	0.102000	0.000000	0.000070	0.725111

0.587277	0.139931	0.005005	0.000055	0.725212
0.588244	0.138411	0.010010	0.000055	0.725210
0.575558	0.143433	0.015014	0.000057	0.725216
0.559476	0.142832	0.020019	0.000060	0.725210
0.685851	0.000982	0.025024	0.000036	0.724977
0.616089	-0.032592	0.030029	0.000049	0.724887
0.479346	-0.010154	0.035034	0.000074	0.724884
0.813309	-0.067724	0.040038	0.000012	0.724888
0.766905	-0.061449	0.045043	0.000020	0.724885
0.625776	-0.035318	0.050048	0.000046	0.724887
0.738366	-0.054076	0.055053	0.000025	0.724890
0.697894	-0.050253	0.060058	0.000032	0.724884
0.828516	-0.069469	0.065062	0.000007	0.724893
0.731237	-0.055652	0.070067	0.000025	0.724886
0.697216	-0.048789	0.075072	0.000031	0.724888
0.707083	-0.050097	0.080077	0.000029	0.724890
0.504229	-0.053390	0.085082	0.000067	0.724813
0.671393	-0.192747	0.090086	0.000035	0.724599
0.566626	-0.177236	0.095091	0.000054	0.724594
0.418729	-0.152213	0.100096	0.000082	0.724592
0.567855	-0.178554	0.105101	0.000054	0.724593
0.662514	-0.198946	0.110106	0.000036	0.724586
0.802804	-0.219327	0.115110	0.000009	0.724596
0.419882	-0.264347	0.120115	0.000080	0.724375
0.386551	-0.318240	0.125120	0.000086	0.724258
0.498118	-0.335902	0.130125	0.000065	0.724263
0.561049	-0.351043	0.135130	0.000053	0.724256
0.466972	-0.330259	0.140134	0.000071	0.724264
0.401779	-0.393894	0.145139	0.000082	0.724117
0.249908	-0.453557	0.150144	0.000111	0.723948
0.465574	-0.490909	0.155149	0.000070	0.723951
0.470984	-0.494852	0.160154	0.000069	0.723945
0.600903	-0.524947	0.165158	0.000044	0.723932
0.431937	-0.649812	0.170163	0.000076	0.723629
0.389079	-0.641456	0.175168	0.000083	0.723631
0.153399	-0.598850	0.180173	0.000127	0.723633
-0.060614	-0.577305	0.185178	0.000166	0.723601
0.201136	-0.756969	0.190182	0.000118	0.723341
0.275310	-0.772436	0.195187	0.000103	0.723337
-0.048175	-0.714594	0.200192	0.000163	0.723338
-0.038229	-0.787091	0.205197	0.000161	0.723200
0.057770	-0.908920	0.210202	0.000143	0.722995
0.135899	-0.919401	0.215206	0.000128	0.723002
0.113305	-0.932400	0.220211	0.000132	0.722969
0.020035	-1.060949	0.225216	0.000149	0.722685
0.101932	-1.073653	0.230221	0.000134	0.722689
0.072802	-1.075021	0.235226	0.000139	0.722677
0.232978	-1.260407	0.240230	0.000109	0.722370
0.159674	-1.251282	0.245235	0.000122	0.722362
-0.152555	-1.217823	0.250240	0.000180	0.722319
-0.011825	-1.369427	0.255245	0.000154	0.722071
-0.041926	-1.367398	0.260250	0.000159	0.722065
-0.323574	-1.380102	0.265254	0.000211	0.721942
-0.562173	-1.441177	0.270259	0.000256	0.721740
-0.674752	-1.421361	0.275264	0.000276	0.721740
-0.283329	-1.578191	0.280269	0.000203	0.721569
-0.512453	-1.608580	0.285274	0.000246	0.721430
-0.410865	-1.625154	0.290278	0.000226	0.721433
-0.402996	-1.786324	0.295283	0.000225	0.721119
-0.740393	-1.727465	0.300288	0.000287	0.721118
-0.705999	-1.788267	0.305293	0.000281	0.721011
-0.864222	-1.830432	0.310298	0.000310	0.720873
-0.853160	-1.828070	0.315302	0.000307	0.720882
-0.945043	-1.981346	0.320307	0.000324	0.720549
-1.071190	-1.966131	0.325312	0.000348	0.720535
-1.191017	-2.022817	0.330317	0.000370	0.720382
-2.289489	-1.913370	0.335322	0.000574	0.720213
-3.377243	-1.715489	0.340326	0.000776	0.720221
-3.756578	-1.715223	0.345331	0.000846	0.720089
-4.149441	-1.747515	0.350336	0.000919	0.719888
-3.971259	-1.775477	0.355341	0.000886	0.719896
-4.414388	-1.702536	0.360346	0.000968	0.719885
-4.675538	-1.722173	0.365350	0.001016	0.719755
-5.079547	-1.733661	0.370355	0.001091	0.719591
-4.957320	-1.754986	0.375360	0.001068	0.719593
-5.325851	-1.687564	0.380365	0.001137	0.719597
-5.518136	-1.659055	0.385370	0.001172	0.719586
-5.505471	-1.819979	0.390374	0.001169	0.719274
-6.245387	-1.694291	0.395379	0.001307	0.719262
-6.698585	-1.612344	0.400384	0.001391	0.719265
-6.044323	-1.727276	0.405389	0.001269	0.719269
-6.243015	-1.696593	0.410394	0.001306	0.719260
-6.714242	-1.759551	0.415398	0.001393	0.718971
-6.942749	-1.725849	0.420403	0.001435	0.718958
-7.349461	-1.655385	0.425408	0.001511	0.718955
-7.180149	-1.683595	0.430413	0.001479	0.718959
-7.160200	-1.689079	0.435418	0.001475	0.718956
-7.033512	-1.783039	0.440422	0.001451	0.718815
-8.370510	-1.633973	0.445427	0.001700	0.718640
-8.162404	-1.672612	0.450432	0.001661	0.718637
-7.818085	-1.731439	0.455437	0.001596	0.718643
-8.138006	-1.677459	0.460442	0.001656	0.718638
-8.193627	-1.662603	0.465446	0.001666	0.718648
-8.080403	-1.739069	0.470451	0.001644	0.718537
-9.056321	-1.660755	0.475456	0.001826	0.718349
-8.706256	-1.720134	0.480461	0.001760	0.718356
-9.325406	-1.615307	0.485466	0.001875	0.718345
-9.024770	-1.665328	0.490470	0.001819	0.718353
-8.933536	-1.683903	0.495475	0.001802	0.718349
-9.383759	-1.606238	0.500480	0.001885	0.718344
-9.488041	-1.736088	0.505485	0.001904	0.718052
-10.015118	-1.664526	0.510490	0.002002	0.718008
-10.030631	-1.657529	0.515494	0.002005	0.718017
-9.828149	-1.695681	0.520499	0.001967	0.718014
-10.207552	-1.630272	0.525504	0.002037	0.718010
-10.176728	-1.631015	0.530509	0.002031	0.718020
-10.212344	-1.629919	0.535514	0.002038	0.718010
-10.210371	-1.774792	0.540518	0.002037	0.717725
-10.974640	-1.651334	0.545523	0.002179	0.717700
-10.997864	-1.648297	0.550528	0.002183	0.717699
-10.386647	-1.752538	0.555533	0.002069	0.717708
-10.764933	-1.691550	0.560538	0.002139	0.717696
-11.030831	-1.640274	0.565542	0.002188	0.717705
-10.804994	-1.737315	0.570547	0.002146	0.717593
-11.533706	-1.716508	0.575552	0.002281	0.717378
-11.483623	-1.723804	0.580557	0.002272	0.717382
-12.051653	-1.627594	0.585562	0.002377	0.717372
-11.575358	-1.709308	0.590566	0.002288	0.717379
-11.546379	-1.718213	0.595571	0.002283	0.717372
-11.977251	-1.641579	0.600576	0.002363	0.717372
-11.754146	-1.754286	0.605581	0.002321	0.717229
-12.715459	-1.659873	0.610586	0.002499	0.717077
-12.392123	-1.715449	0.615590	0.002439	0.717082
-12.508851	-1.697768	0.620595	0.002460	0.717076
-12.824018	-1.642807	0.625600	0.002519	0.717074
-12.619791	-1.677088	0.630605	0.002481	0.717079
-13.008918	-1.610254	0.635610	0.002553	0.717075
-12.763869	-1.722737	0.640614	0.002507	0.716939
-14.027160	-1.593860	0.645619	0.002742	0.716749
-13.941662	-1.608137	0.650624	0.002725	0.716752
-13.514657	-1.681156	0.655629	0.002646	0.716758
-13.770472	-1.640197	0.660634	0.002693	0.716750
-13.799958	-1.633046	0.665638	0.002698	0.716754
-13.931583	-1.610817	0.670643	0.002722	0.716752
-13.617436	-1.667124	0.675648	0.002664	0.716752
-13.407653	-1.800261	0.680653	0.002624	0.716563
-14.976082	-1.583745	0.685658	0.002916	0.716439
-14.576131	-1.650648	0.690662	0.002841	0.716448
-14.386742	-1.688005	0.695667	0.002806	0.716441
-15.036029	-1.573010	0.700672	0.002926	0.716441
-14.645548	-1.639369	0.705677	0.002853	0.716448
-14.495215	-1.669060	0.710682	0.002825	0.716442
-14.520226	-1.716704	0.715686	0.002830	0.716340
-15.607005	-1.630208	0.720691	0.003032	0.716128
-15.449966	-1.658452	0.725696	0.003002	0.716128
-15.560368	-1.635983	0.730701	0.003022	0.716134
-15.761796	-1.605888	0.735706	0.003060	0.716123
-15.380283	-1.671755	0.740710	0.002988	0.716128
-15.358392	-1.675492	0.745715	0.002984	0.716129
-15.543914	-1.642675	0.750720	0.003018	0.716129
-15.814257	-1.714459	0.755725	0.003068	0.715892
-16.152032	-1.663341	0.760730	0.003131	0.715874
-16.331552	-1.627733	0.765734	0.003164	0.715882
-16.431320	-1.610743	0.770739	0.003182	0.715881
-16.416671	-1.616222	0.775744	0.003179	0.715876
-16.243939	-1.642616	0.780749	0.003147	0.715885
-16.635224	-1.576728	0.785754	0.003219	0.715878
-16.937982	-1.679147	0.790758	0.003276	0.715569
-17.144428	-1.655198	0.795763	0.003314	0.715544
-17.515085	-1.589399	0.800768	0.003382	0.715544
-17.096922	-1.662391	0.805773	0.003304	0.715547
-17.490124	-1.597772	0.810778	0.003377	0.715537
-17.198252	-1.646770	0.815782	0.003323	0.715544
-17.283441	-1.634581	0.820787	0.003338	0.715538
-17.581266	-1.689440	0.825792	0.003393	0.715325
-18.115377	-1.641662	0.830797	0.003492	0.715231
-18.310173	-1.611755	0.835802	0.003528	0.715222
-18.093066	-1.647122	0.840806	0.003488	0.715229
-18.103226	-1.647943	0.845811	0.003489	0.715225
-18.530493	-1.573002	0.850816	0.003569	0.715223
-18.112101	-1.644070	0.855821	0.003490	0.715230
-18.107293	-1.713063	0.860826	0.003489	0.715096
-19.184614	-1.618169	0.865830	0.003690	0.714904
-18.989059	-1.652413	0.870835	0.003653	0.714906
-19.427298	-1.577127	0.875840	0.003734	0.714901
-18.991964	-1.652160	0.880845	0.003653	0.714906
-19.243448	-1.609792	0.885850	0.003699	0.714902
-19.443035	-1.572303	0.890854	0.003736	0.714906
-19.209822	-1.613373	0.895859	0.003693	0.714908
-19.760391	-1.666938	0.900864	0.003795	0.714607
-20.052022	-1.613720	0.905869	0.003849	0.714610
-20.347593	-1.566010	0.910874	0.003904	0.714601
-19.735974	-1.672020	0.915878	0.003789	0.714607
-20.018955	-1.620933	0.920883	0.003842	0.714609
-20.033229	-1.621805	0.925888	0.003844	0.714603
-19.531722	-1.709810	0.930893	0.003751	0.714606
-20.850475	-1.636075	0.935898	0.003996	0.714286
-21.020657	-1.611880	0.940902	0.004027	0.714275
-20.735379	-1.663054	0.945907	0.003974	0.714275
-20.958872	-1.624804	0.950912	0.004015	0.714272
-21.006690	-1.611369	0.955917	0.004024	0.714282
-21.060237	-1.609604	0.960922	0.004033	0.714268
-20.762580	-1.658111	0.965926	0.003978	0.714277
-21.013014	-1.704202	0.970931	0.004024	0.714097
-22.244055	-1.552822	0.975936	0.004253	0.713963
-21.349388	-1.710486	0.980941	0.004086	0.713967
-21.886307	-1.617101	0.985946	0.004186	0.713963
-22.119305	-1.573581	0.990950	0.004229	0.713967
-21.586866	-1.670519	0.995955	0.004130	0.713964
-21.859774	-1.623307	1.000960	0.004180	0.713962
-21.994899	-1.662923	1.005965	0.004205	0.713836
-22.915259	-1.595249	1.010970	0.004376	0.713645
-22.655704	-1.639918	1.015974	0.004327	0.713648
-22.924010	-1.592150	1.020979	0.004377	0.713649
-22.989560	-1.582586	1.025984	0.004389	0.713645
-22.553582	-1.655470	1.030989	0.004308	0.713655
-22.907389	-1.597375	1.035994	0.004373	0.713646
-22.927557	-1.591736	1.040998	0.004377	0.713650
-22.914309	-1.723493	1.046003	0.004374	0.713394
-23.589414	-1.623963	1.051008	0.004499	0.713353
-23.666647	-1.608354	1.056013	0.004513	0.713357
-23.449618	-1.651295	1.061018	0.004473	0.713349
-23.560353	-1.628932	1.066022	0.004493	0.713355
-23.748038	-1.596782	1.071027	0.004528	0.713353
-23.789749	-1.590563	1.076032	0.004535	0.713351
-23.637344	-1.767807	1.081037	0.004507	0.713053
-24.460854	-1.641429	1.086042	0.004660	0.713013
-24.887323	-1.561556	1.091046	0.004739	0.713021
-24.247570	-1.677030	1.096051	0.004619	0.713019
-24.389737	-1.653343	1.101056	0.004645	0.713016
-24.423486	-1.644776	1.106061	0.004651	0.713022
-24.501977	-1.644082	1.111066	0.004666	0.712996
-25.073664	-1.686626	1.116070	0.004772	0.712709
-25.188504	-1.668394	1.121075	0.004793	0.712705
-25.476896	-1.618220	1.126080	0.004846	0.712703
-25.196420	-1.663526	1.131085	0.004794	0.712713
-25.416189	-1.630832	1.136090	0.004835	0.712701
-25.652543	-1.585539	1.141094	0.004878	0.712708
-25.028930	-1.710802	1.146099	0.004762	0.712680
-26.041702	-1.681149	1.151104	0.004950	0.712380
-26.514008	-1.593971	1.156109	0.005038	0.712387
-26.532345	-1.594775	1.161114	0.005041	0.712379
-26.076848	-1.672955	1.166118	0.004956	0.712386
-26.438823	-1.609824	1.171123	0.005023	0.712383
-27.019427	-1.511225	1.176128	0.005131	0.712374
-26.083679	-1.672471	1.181133	0.004956	0.712386
-26.134470	-1.747101	1.186138	0.004966	0.712220
-27.679740	-1.537517	1.191142	0.005253	0.712089
-27.367369	-1.594584	1.196147	0.005195	0.712087
-27.296982	-1.608924	1.201152	0.005181	0.712084
-27.118509	-1.637197	1.206157	0.005148	0.712091
-27.446435	-1.583970	1.211162	0.005208	0.712081
-27.366482	-1.594531	1.216166	0.005193	0.712089
-27.434495	-1.585934	1.221171	0.005206	0.712083
-28.051548	-1.640314	1.226176	0.005320	0.711756
-28.079548	-1.632228	1.231181	0.005325	0.711763
-28.321488	-1.592832	1.236186	0.005370	0.711756
-28.175452	-1.616815	1.241190	0.005342	0.711760
-27.949126	-1.658981	1.246195	0.005300	0.711757
-28.180611	-1.620156	1.251200	0.005343	0.711753
-28.229743	-1.607326	1.256205	0.005352	0.711762
-28.674257	-1.638528	1.261210	0.005434	0.711542
-29.132728	-1.603316	1.266214	0.005519	0.711450
-28.789951	-1.664980	1.271219	0.005455	0.711449
-29.297002	-1.577714	1.276224	0.005549	0.711444
-29.372906	-1.559216	1.281229	0.005563	0.711454
-28.858600	-1.656063	1.286234	0.005467	0.711444
-29.206133	-1.589514	1.291238	0.005532	0.711454
-29.133117	-1.662227	1.296243	0.005518	0.711335
-29.853870	-1.636233	1.301248	0.005652	0.711131
-29.535350	-1.690290	1.306253	0.005592	0.711137
-29.880596	-1.632167	1.311258	0.005656	0.711131
-29.705890	-1.662397	1.316262	0.005623	0.711134
-29.523134	-1.694491	1.321267	0.005589	0.711135
-30.199902	-1.576274	1.326272	0.005715	0.711131
-30.048988	-1.702568	1.331277	0.005686	0.710933
-30.395128	-1.676382	1.336282	0.005750	0.710863
-30.556040	-1.643716	1.341286	0.005780	0.710871
-30.491772	-1.656260	1.346291	0.005768	0.710869
-30.512707	-1.656084	1.351296	0.005771	0.710863
-30.521345	-1.650163	1.356301	0.005773	0.710872
-30.643282	-1.698287	1.361306	0.005795	0.710733
-31.475853	-1.650590	1.366310	0.005950	0.710533
-30.933276	-1.749231	1.371315	0.005849	0.710529
-31.472205	-1.654282	1.376320	0.005949	0.710528
-31.633250	-1.622649	1.381325	0.005978	0.710534
-31.046738	-1.730683	1.386330	0.005869	0.710528
-31.249701	-1.695292	1.391334	0.005906	0.710527
-32.238048	-1.673862	1.396339	0.006090	0.710218
-32.411741	-1.646538	1.401344	0.006122	0.710211
-32.341913	-1.656284	1.406349	0.006109	0.710217
-32.400107	-1.650792	1.411354	0.006119	0.710208
-32.706715	-1.593610	1.416358	0.006176	0.710214
-32.542878	-1.621945	1.421363	0.006145	0.710216
-32.316813	-1.665159	1.426368	0.006103	0.710211
-32.534397	-1.734864	1.431373	0.006143	0.709994
-33.584447	-1.600903	1.436378	0.006339	0.709889
-33.378278	-1.636433	1.441382	0.006300	0.709892
-33.501457	-1.614126	1.446387	0.006323	0.709893
-33.784468	-1.567630	1.451392	0.006375	0.709886
-33.245850	-1.658815	1.456397	0.006274	0.709896
-33.577492	-1.603964	1.461402	0.006336	0.709888
-33.572909	-1.623438	1.466406	0.006335	0.709851
-33.885240	-1.695593	1.471411	0.006393	0.709596
-34.374324	-1.612602	1.476416	0.006483	0.709588
-34.464940	-1.591807	1.481421	0.006500	0.709598
-34.081304	-1.666418	1.486426	0.006428	0.709586
-33.861245	-1.703293	1.491430	0.006387	0.709591
-34.458137	-1.597382	1.496435	0.006498	0.709591
-34.297438	-1.649587	1.501440	0.006468	0.709544
-34.662032	-1.724304	1.506445	0.006535	0.709265
-34.997797	-1.669532	1.511450	0.006598	0.709256
-35.505948	-1.577834	1.516454	0.006692	0.709259
-35.131519	-1.643354	1.521459	0.006622	0.709261
-35.123496	-1.647629	1.526464	0.006620	0.709256
-35.217926	-1.627053	1.531469	0.006637	0.709264
-35.387979	-1.601228	1.536474	0.006669	0.709256
-35.496574	-1.719755	1.541478	0.006689	0.708980
-36.341849	-1.584932	1.546483	0.006846	0.708949
-36.477477	-1.562940	1.551488	0.006871	0.708946
-35.829119	-1.675139	1.556493	0.006750	0.708953
-35.937505	-1.658704	1.561498	0.006770	0.708948
-36.231943	-1.605368	1.566502	0.006824	0.708950
-35.901855	-1.666340	1.571507	0.006762	0.708946
-36.264270	-1.712482	1.576512	0.006830	0.708725
-37.325032	-1.566755	1.581517	0.007027	0.708639
-37.035876	-1.623627	1.586522	0.006973	0.708628
-36.801517	-1.662940	1.591526	0.006929	0.708634
-37.266144	-1.581140	1.596531	0.007015	0.708632
-37.352873	-1.568837	1.601536	0.007031	0.708627
-36.798257	-1.661059	1.606541	0.006927	0.708641
-37.113409	-1.640034	1.611546	0.006986	0.708571
-37.988844	-1.597285	1.616550	0.007149	0.708344
-37.465723	-1.689897	1.621555	0.007051	0.708346
-37.841045	-1.627402	1.626560	0.007120	0.708338
-37.663039	-1.655309	1.631565	0.007087	0.708346
-37.742314	-1.645891	1.636570	0.007101	0.708337
-37.687023	-1.652666	1.641574	0.007091	0.708344
-37.926007	-1.688660	1.646579	0.007135	0.708187
-39.178253	-1.556805	1.651584	0.007368	0.708004
-38.182544	-1.731628	1.656589	0.007182	0.708010
-38.814175	-1.623133	1.661594	0.007300	0.708002
-39.196665	-1.554023	1.666598	0.007371	0.708005
-38.411141	-1.692824	1.671603	0.007224	0.708008
-38.708732	-1.643479	1.676608	0.007279	0.708001
-38.957222	-1.637569	1.681613	0.007325	0.707925
-39.834033	-1.598118	1.686618	0.007488	0.707691
-39.255170	-1.700904	1.691622	0.007380	0.707692
-39.649799	-1.630991	1.696627	0.007453	0.707692
-39.972091	-1.576151	1.701632	0.007513	0.707687
-39.490829	-1.655820	1.706637	0.007423	0.707700
-39.489570	-1.661296	1.711642	0.007423	0.707690
-39.483059	-1.691793	1.716646	0.007421	0.707632
-40.312828	-1.673082	1.721651	0.007575	0.707373
-40.468172	-1.649825	1.726656	0.007604	0.707365
-40.662919	-1.610482	1.731661	0.007640	0.707374
-40.645291	-1.617395	1.736666	0.007636	0.707367
-40.462298	-1.647055	1.741670	0.007602	0.707374
-40.322142	-1.673085	1.746675	0.007576	0.707372
-40.697412	-1.615800	1.751680	0.007645	0.707354
-41.076842	-1.684729	1.756685	0.007716	0.707080
-41.399912	-1.630368	1.761690	0.007775	0.707074
-41.735872	-1.569199	1.766694	0.007838	0.707077
-41.201647	-1.665588	1.771699	0.007738	0.707075
-41.256974	-1.657746	1.776704	0.007748	0.707072
-41.529819	-1.606933	1.781709	0.007799	0.707077
-41.665927	-1.585742	1.786714	0.007824	0.707071
-41.707211	-1.714577	1.791718	0.007831	0.706798
-42.487985	-1.601280	1.796723	0.007976	0.706747
-42.754570	-1.556673	1.801728	0.008025	0.706742
-42.100431	-1.668417	1.806733	0.007903	0.706752
-42.137158	-1.666765	1.811738	0.007910	0.706743
-42.448416	-1.609688	1.816742	0.007968	0.706746
-42.275503	-1.641053	1.821747	0.007935	0.706746
-42.759757	-1.658037	1.826752	0.008025	0.706539
-43.257783	-1.617736	1.831757	0.008117	0.706442
-43.386270	-1.600151	1.836762	0.008141	0.706432
-43.246934	-1.623085	1.841766	0.008115	0.706436
-43.188219	-1.632423	1.846771	0.008104	0.706439
-43.485509	-1.585642	1.851776	0.008159	0.706427
-43.169473	-1.634364	1.856781	0.008100	0.706443
-43.310088	-1.657766	1.861786	0.008126	0.706346
-44.142727	-1.622484	1.866790	0.008280	0.706119
-43.686260	-1.701718	1.871795	0.008195	0.706124
-44.244079	-1.605385	1.876800	0.008299	0.706118
-43.843322	-1.673601	1.881805	0.008224	0.706125
-44.031580	-1.643108	1.886810	0.008258	0.706120
-43.940185	-1.658156	1.891814	0.008241	0.706123
-43.842729	-1.759256	1.896819	0.008223	0.705955
-45.332461	-1.546160	1.901824	0.008500	0.705850
-44.962633	-1.608167	1.906829	0.008431	0.705858
-44.568288	-1.681839	1.911834	0.008357	0.705852
-44.715436	-1.654831	1.916838	0.008384	0.705854
-45.070435	-1.591003	1.921843	0.008450	0.705856
-45.077863	-1.593209	1.926848	0.008451	0.705849
-45.051230	-1.716759	1.931853	0.008446	0.705611
-46.109219	-1.574467	1.936858	0.008642	0.705518
-45.813442	-1.626612	1.941862	0.008587	0.705520
-45.405195	-1.698613	1.946867	0.008511	0.705522
-45.978663	-1.600997	1.951872	0.008617	0.705513
-45.609499	-1.662152	1.956877	0.008548	0.705523
-45.683390	-1.653788	1.961882	0.008562	0.705514
-46.385958	-1.665197	1.966886	0.008692	0.705240
-46.681239	-1.628257	1.971891	0.008747	0.705208
-46.849791	-1.602822	1.976896	0.008778	0.705200
-46.380251	-1.681099	1.981901	0.008690	0.705211
-46.968290	-1.580067	1.986906	0.008800	0.705204
-46.866392	-1.596371	1.991910	0.008780	0.705208
-46.338364	-1.690658	1.996915	0.008682	0.705209
-47.294726	-1.662991	2.001920	0.008860	0.704922

-47.265704	-1.687757	2.011917	0.008854	0.704883
-47.804214	-1.592100	2.021914	0.008953	0.704884
-47.562973	-1.634678	2.031910	0.008908	0.704886
-47.546572	-1.636745	2.041907	0.008904	0.704888
-47.771903	-1.598162	2.051904	0.008946	0.704886
-47.542666	-1.640889	2.061901	0.008902	0.704884
-47.740423	-1.607377	2.071898	0.008939	0.704881
-47.491527	-1.651281	2.081894	0.008892	0.704883
-47.572707	-1.636302	2.091891	0.008906	0.704885
-47.626363	-1.627781	2.101888	0.008916	0.704884
-47.551857	-1.642652	2.111885	0.008901	0.704882
-47.059243	-1.596894	2.121882	0.008809	0.705152
-46.484192	-1.672972	2.131878	0.008701	0.705207
-46.479451	-1.674474	2.141875	0.008700	0.705206
-46.466155	-1.677618	2.151872	0.008697	0.705206
-46.513617	-1.671949	2.161869	0.008705	0.705201
-46.459259	-1.680627	2.171866	0.008694	0.705204
-45.872574	-1.688385	2.181862	0.008585	0.705400
-45.555531	-1.686417	2.191859	0.008525	0.705519
-45.688009	-1.662331	2.201856	0.008549	0.705521
-45.622659	-1.676036	2.211853	0.008536	0.705518
-45.810058	-1.616954	2.221850	0.008571	0.705571
-44.842914	-1.649546	2.231846	0.008390	0.705853
-44.843859	-1.648053	2.241843	0.008390	0.705857
-44.987099	-1.625779	2.251840	0.008416	0.705852
-44.706037	-1.632046	2.261837	0.008363	0.705941
-43.994046	-1.670660	2.271834	0.008230	0.706120
-43.933834	-1.680729	2.281830	0.008218	0.706122
-44.229634	-1.627917	2.291827	0.008272	0.706123
-43.626669	-1.620552	2.301824	0.008160	0.706355
-43.415256	-1.618375	2.311821	0.008120	0.706436
-43.268228	-1.644852	2.321818	0.008092	0.706437
-42.970136	-1.646880	2.331814	0.008036	0.706541
-42.528686	-1.623372	2.341811	0.007953	0.706747
-42.350220	-1.655024	2.351808	0.007919	0.706748
-42.482228	-1.634018	2.361805	0.007943	0.706745
-41.886801	-1.595850	2.371802	0.007832	0.707035
-41.419978	-1.660450	2.381798	0.007744	0.707074
-41.418721	-1.659346	2.391795	0.007743	0.707078
-41.324273	-1.635574	2.401792	0.007725	0.707160
-40.747042	-1.634769	2.411789	0.007617	0.707369
-40.745054	-1.636287	2.421786	0.007616	0.707368
-40.955306	-1.588914	2.431782	0.007655	0.707389
-40.147020	-1.582077	2.441779	0.007504	0.707693
-39.752490	-1.653445	2.451776	0.007430	0.707692
-39.860993	-1.635932	2.461773	0.007449	0.707689
-39.420522	-1.611523	2.471770	0.007367	0.707897
-38.839252	-1.660320	2.481766	0.007258	0.708008
-39.204801	-1.595745	2.491763	0.007325	0.708008
-38.997057	-1.594643	2.501760	0.007286	0.708085
-38.226304	-1.605757	2.511757	0.007142	0.708339
-37.865891	-1.669131	2.521754	0.007075	0.708342
-38.199123	-1.609927	2.531750	0.007136	0.708343
-37.570568	-1.615153	2.541747	0.007018	0.708558
-37.230106	-1.638726	2.551744	0.006954	0.708633
-37.164461	-1.653112	2.561741	0.006942	0.708629
-37.199598	-1.614420	2.571738	0.006948	0.708695
-36.529289	-1.606380	2.581734	0.006822	0.708952
-36.551648	-1.603247	2.591731	0.006826	0.708951
-36.366061	-1.639167	2.601728	0.006791	0.708946
-36.077169	-1.549120	2.611725	0.006736	0.709231
-35.479527	-1.644419	2.621722	0.006625	0.709254
-35.548612	-1.631085	2.631718	0.006637	0.709257
-35.166314	-1.614028	2.641715	0.006565	0.709429
-34.630423	-1.630301	2.651712	0.006465	0.709588
-34.905796	-1.580241	2.661709	0.006515	0.709592
-34.537229	-1.636698	2.671706	0.006446	0.709611
-34.037297	-1.587989	2.681702	0.006353	0.709888
-33.845485	-1.621814	2.691699	0.006316	0.709890
-33.856540	-1.621792	2.701696	0.006318	0.709887
-33.434443	-1.587503	2.711693	0.006239	0.710107
-33.005040	-1.612442	2.721690	0.006158	0.710211
-33.135790	-1.588626	2.731686	0.006182	0.710213
-32.781559	-1.609390	2.741683	0.006115	0.710299
-32.299949	-1.582587	2.751680	0.006025	0.710525
-32.123975	-1.614956	2.761677	0.005992	0.710524
-31.990129	-1.640170	2.771674	0.005966	0.710522
-31.359711	-1.609865	2.781670	0.005848	0.710808
-31.073230	-1.632725	2.791667	0.005794	0.710866
-31.027439	-1.642796	2.801664	0.005785	0.710863
-31.023510	-1.636833	2.811661	0.005784	0.710877
-30.435090	-1.615610	2.821658	0.005674	0.711130
-30.305450	-1.637450	2.831654	0.005649	0.711133
-30.226422	-1.652465	2.841651	0.005634	0.711133
-30.132532	-1.570215	2.851648	0.005616	0.711331
-29.644417	-1.601363	2.861645	0.005524	0.711444
-29.740919	-1.584628	2.871642	0.005542	0.711444
-29.661621	-1.531514	2.881638	0.005526	0.711579
-28.573331	-1.639250	2.891635	0.005323	0.711752
-28.864384	-1.587104	2.901632	0.005377	0.711754
-28.751562	-1.584582	2.911629	0.005355	0.711800
-27.797840	-1.614940	2.921626	0.005177	0.712079
-27.793239	-1.615005	2.931622	0.005176	0.712082
-27.673788	-1.636124	2.941619	0.005153	0.712083
-27.566139	-1.559285	2.951616	0.005132	0.712276
-26.775139	-1.648868	2.961613	0.004985	0.712379
-27.034990	-1.604206	2.971610	0.005032	0.712377
-26.972518	-1.582019	2.981606	0.005020	0.712444
-25.870659	-1.650916	2.991603	0.004814	0.712699
-26.146825	-1.601699	3.001600	0.004865	0.712700
-26.216779	-1.590011	3.011597	0.004878	0.712700
-25.667844	-1.567171	3.021594	0.004775	0.712941
-25.306045	-1.595578	3.031590	0.004707	0.713014
-25.295468	-1.597728	3.041587	0.004705	0.713014
-25.072735	-1.571504	3.051584	0.004662	0.713147
-24.138455	-1.635391	3.061581	0.004488	0.713352
-24.398914	-1.589250	3.071578	0.004536	0.713352
-24.269343	-1.611815	3.081574	0.004511	0.713354
-23.713029	-1.594452	3.091571	0.004407	0.713587
-23.577773	-1.590045	3.101568	0.004381	0.713645
-23.288303	-1.642552	3.111565	0.004327	0.713644
-23.534086	-1.553115	3.121562	0.004372	0.713736
-22.370640	-1.646252	3.131558	0.004155	0.713964
-22.594315	-1.606352	3.141555	0.004196	0.713965
-22.505422	-1.623595	3.151552	0.004179	0.713963
-22.036877	-1.587339	3.161549	0.004091	0.714202
-21.952952	-1.568527	3.171546	0.004075	0.714270
-21.680107	-1.616929	3.181542	0.004023	0.714272
-21.552744	-1.578389	3.191539	0.003999	0.714395
-20.940856	-1.583691	3.201536	0.003885	0.714602
-20.815568	-1.607103	3.211533	0.003861	0.714601
-21.022997	-1.571239	3.221530	0.003899	0.714599
-20.033572	-1.599431	3.231526	0.003714	0.714894
-20.082326	-1.585773	3.241523	0.003723	0.714905
-20.001956	-1.602757	3.251520	0.003707	0.714901
-19.768948	-1.553637	3.261517	0.003663	0.715082
-19.123536	-1.596753	3.271514	0.003542	0.715226
-19.074926	-1.606622	3.281510	0.003533	0.715224
-19.086534	-1.604149	3.291507	0.003534	0.715226
-18.334373	-1.583622	3.301504	0.003394	0.715534
-18.119267	-1.620590	3.311501	0.003353	0.715538
-18.286205	-1.591076	3.321498	0.003384	0.715538
-17.977968	-1.574035	3.331494	0.003326	0.715682
-17.295242	-1.595693	3.341491	0.003198	0.715881
-17.461877	-1.567692	3.351488	0.003228	0.715879
-17.457238	-1.570281	3.361485	0.003227	0.715876
-16.730106	-1.575243	3.371482	0.003091	0.716124
-16.498092	-1.615338	3.381478	0.003047	0.716128
-16.495975	-1.616098	3.391475	0.003046	0.716128
-16.255430	-1.565271	3.401472	0.003001	0.716315
-15.733898	-1.594072	3.411469	0.002903	0.716443
-15.872817	-1.571248	3.421466	0.002929	0.716440
-15.319322	-1.641768	3.431462	0.002825	0.716497
-14.772178	-1.609850	3.441459	0.002723	0.716754
-14.577148	-1.645683	3.451456	0.002686	0.716753
-14.751010	-1.615688	3.461453	0.002717	0.716752
-14.271473	-1.629500	3.471450	0.002628	0.716895
-13.500933	-1.672022	3.481446	0.002484	0.717083
-13.786195	-1.622896	3.491443	0.002536	0.717081
-13.616440	-1.654542	3.501440	0.002504	0.717079
-13.203578	-1.618902	3.511437	0.002427	0.717296
-12.907563	-1.634705	3.521434	0.002371	0.717370
-12.541231	-1.699508	3.531430	0.002302	0.717372
-12.802546	-1.651527	3.541427	0.002350	0.717376
-11.925076	-1.645614	3.551424	0.002186	0.717698
-11.988794	-1.635635	3.561421	0.002197	0.717696
-11.799937	-1.670604	3.571418	0.002162	0.717695
-11.872602	-1.595447	3.581414	0.002175	0.717819
-10.753814	-1.697405	3.591411	0.001966	0.718012
-10.875346	-1.675073	3.601408	0.001988	0.718015
-10.873823	-1.677150	3.611405	0.001987	0.718012
-10.603105	-1.624150	3.621402	0.001936	0.718213
-9.866403	-1.686333	3.631398	0.001798	0.718350
-10.090054	-1.646841	3.641395	0.001839	0.718351
-9.790247	-1.700621	3.651392	0.001783	0.718351
-9.232085	-1.671526	3.661389	0.001679	0.718606
-9.183582	-1.663244	3.671386	0.001669	0.718640
-9.198131	-1.660559	3.681382	0.001671	0.718642
-8.992910	-1.642965	3.691379	0.001632	0.718750
-8.119426	-1.694513	3.701376	0.001469	0.718956
-8.443218	-1.636236	3.711373	0.001529	0.718958
-8.032248	-1.709535	3.721370	0.001452	0.718959
-7.639725	-1.673685	3.731366	0.001378	0.719169
-7.200616	-1.702300	3.741363	0.001296	0.719268
-7.404463	-1.665624	3.751360	0.001333	0.719269
-7.308774	-1.677023	3.761357	0.001315	0.719281
-6.559358	-1.652032	3.771354	0.001175	0.719595
-6.604581	-1.643249	3.781350	0.001183	0.719597
-6.294942	-1.699013	3.791347	0.001124	0.719597
-5.984854	-1.674913	3.801344	0.001066	0.719755
-5.598662	-1.673075	3.811341	0.000994	0.719895
-5.539168	-1.685360	3.821338	0.000982	0.719893
-5.639490	-1.666288	3.831334	0.001000	0.719896
-4.764217	-1.659872	3.841331	0.000836	0.720217
-4.625634	-1.683385	3.851328	0.000810	0.720220
-4.781648	-1.656339	3.861325	0.000839	0.720220
-4.433213	-1.648401	3.871322	0.000773	0.720359
-3.958312	-1.642563	3.881318	0.000684	0.720538
-4.040865	-1.628322	3.891315	0.000699	0.720538
-3.888643	-1.638023	3.901312	0.000670	0.720573
-3.537803	-1.549252	3.911309	0.000604	0.720872
-3.423200	-1.569008	3.921306	0.000582	0.720874
-3.392998	-1.557726	3.931302	0.000576	0.720908
-2.953768	-1.529208	3.941299	0.000494	0.721119
-2.953263	-1.529639	3.951296	0.000493	0.721119
-2.955085	-1.462097	3.961293	0.000493	0.721253
-2.720441	-1.413076	3.971290	0.000448	0.721432
-2.473263	-1.457591	3.981286	0.000402	0.721432
-2.393073	-1.326164	3.991283	0.000386	0.721720
-2.204418	-1.349757	4.001280	0.000351	0.721740
-1.929170	-1.292187	4.011277	0.000299	0.721951
-2.088449	-1.203133	4.021274	0.000328	0.722071
-2.002409	-1.138210	4.031270	0.000311	0.722230
-1.758360	-1.112749	4.041267	0.000265	0.722366
-1.780904	-1.014722	4.051264	0.000269	0.722552
-1.730591	-0.954733	4.061261	0.000259	0.722688
-1.866145	-0.803876	4.071258	0.000283	0.722938
-1.206808	-0.865674	4.081254	0.000160	0.723048
-1.366425	-0.688107	4.091251	0.000189	0.723342
-1.128254	-0.653076	4.101248	0.000144	0.723494
-0.959701	-0.612770	4.111245	0.000112	0.723633
-0.993809	-0.457507	4.121242	0.000118	0.723927
-0.954093	-0.384085	4.131238	0.000110	0.724085
-0.924249	-0.292444	4.141235	0.000104	0.724276
-0.715113	-0.169053	4.151232	0.000064	0.724592
-0.693666	-0.069498	4.161229	0.000059	0.724795
-0.647342	0.032091	4.171226	0.000050	0.725011
-0.416134	0.114348	4.181222	0.000007	0.725253
0.000000	0.231206	4.191219	-0.000072	0.725628

0.189862	0.794119	4.196224	-0.000108	0.726794
0.573082	2.018287	4.201229	-0.000180	0.729311
1.283377	3.772571	4.206234	-0.000314	0.732960
2.144902	6.055225	4.211238	-0.000476	0.737658
3.079818	8.857323	4.216243	-0.000652	0.743343
4.051686	12.143429	4.221248	-0.000835	0.749912
5.319576	15.841225	4.226253	-0.001074	0.757294
6.912248	19.909672	4.231258	-0.001374	0.765398
8.803991	24.330109	4.236262	-0.001729	0.774159
10.466189	29.168332	4.241267	-0.002042	0.783503
11.500073	34.481587	4.246272	-0.002238	0.793387
12.619694	40.089542	4.251277	-0.002451	0.803696
13.974816	45.981987	4.256282	-0.002707	0.814441
14.627579	52.261165	4.261286	-0.002833	0.825497
15.386025	58.817366	4.266291	-0.002979	0.836907
16.287037	65.537963	4.271296	-0.003151	0.848480
17.048557	72.513767	4.276301	-0.003298	0.860277
17.593718	79.736703	4.281306	-0.003404	0.872254
18.218673	87.107284	4.286310	-0.003526	0.884327
19.354107	94.584217	4.291315	-0.003742	0.896548
20.111527	102.273957	4.296320	-0.003889	0.908831
20.743072	110.124064	4.301325	-0.004012	0.921164
21.638144	118.039546	4.306330	-0.004184	0.933502
22.468804	126.071041	4.311334	-0.004344	0.945836
23.336340	134.215956	4.316339	-0.004511	0.958188
24.052073	142.460200	4.321344	-0.004650	0.970488
24.399053	150.832147	4.326349	-0.004720	0.982726
25.151471	159.260601	4.331354	-0.004866	0.994993
25.869927	167.674621	4.336358	-0.005006	1.007083
27.281614	176.045702	4.341363	-0.005274	1.019136
28.054921	184.567648	4.346368	-0.005424	1.031103
28.815606	193.114583	4.351373	-0.005572	1.042963
29.713141	201.688394	4.356378	-0.005745	1.054757
30.473191	210.293176	4.361382	-0.005892	1.066429
30.846541	219.000566	4.366387	-0.005968	1.078022
31.465934	227.641309	4.371392	-0.006089	1.089460
32.237216	236.275976	4.376397	-0.006238	1.100804
32.877009	244.945463	4.381402	-0.006364	1.112048
33.640443	253.570181	4.386406	-0.006512	1.123150
34.694421	262.166890	4.391411	-0.006714	1.134169
35.167949	270.841983	4.396416	-0.006808	1.145056
35.425213	279.589112	4.401421	-0.006862	1.155883
35.696503	288.263106	4.406426	-0.006918	1.166523
36.370760	296.851921	4.411430	-0.007050	1.177048
37.118722	305.436054	4.416435	-0.007195	1.187488
37.963567	313.996678	4.421440	-0.007358	1.197828
38.337554	322.615723	4.426445	-0.007433	1.208054
38.859374	331.211691	4.431450	-0.007536	1.218197
39.425833	339.774604	4.436454	-0.007648	1.228226
39.959852	348.347955	4.441459	-0.007753	1.238179
40.383238	356.890757	4.446464	-0.007838	1.247997
40.690814	365.457678	4.451469	-0.007901	1.257743
41.270001	373.955639	4.456474	-0.008015	1.267387
41.624925	382.476427	4.461478	-0.008087	1.276943
41.981611	390.983349	4.466483	-0.008159	1.286412
42.671863	399.425933	4.471488	-0.008293	1.295803
43.066997	407.902411	4.476493	-0.008372	1.305108
43.564477	416.472564	4.481498	-0.008471	1.314468
43.743465	424.940438	4.486502	-0.008510	1.323594
44.460271	433.316000	4.491507	-0.008649	1.332655
44.771259	441.736213	4.496512	-0.008713	1.341630
45.224439	450.124574	4.501517	-0.008803	1.350537
46.012778	458.465902	4.506522	-0.008956	1.359395
46.688780	466.801148	4.511526	-0.009087	1.368169
47.106112	475.202356	4.516531	-0.009171	1.376911
47.523590	483.570172	4.521536	-0.009254	1.385563
47.765803	491.983080	4.526541	-0.009305	1.394177
48.751836	500.236303	4.531546	-0.009494	1.402702
48.937030	508.617842	4.536550	-0.009534	1.411171
49.324738	516.975155	4.541555	-0.009612	1.419598
50.085095	525.248837	4.546560	-0.009760	1.427953
50.679756	533.563214	4.551565	-0.009876	1.436273
51.230143	541.868571	4.556570	-0.009984	1.444529
51.743782	550.183178	4.561574	-0.010086	1.452740
52.121381	558.504529	4.566579	-0.010162	1.460890
52.387332	566.853384	4.571584	-0.010217	1.469003
52.749366	575.192712	4.576589	-0.010290	1.477078
53.214357	583.452358	4.581594	-0.010382	1.485049
53.639185	591.723315	4.586598	-0.010467	1.492982
54.416540	599.939452	4.591603	-0.010617	1.500875
55.006714	608.196682	4.596608	-0.010733	1.508736
55.406258	616.483392	4.601613	-0.010813	1.516555
56.014644	624.713592	4.606618	-0.010932	1.524313
56.238493	633.015777	4.611622	-0.010979	1.532039
56.620810	641.284262	4.616627	-0.011056	1.539720
56.899491	649.549798	4.621632	-0.011114	1.547345
57.391756	657.808726	4.626637	-0.011211	1.554957
57.917939	666.021653	4.631642	-0.011315	1.562495
58.259180	674.259289	4.636646	-0.011384	1.569993
58.811056	682.489400	4.641651	-0.011492	1.577478
59.265648	690.690419	4.646656	-0.011583	1.584888
59.529785	698.949473	4.651661	-0.011637	1.592287
60.111852	707.138897	4.656666	-0.011751	1.599636
60.468428	715.346034	4.661670	-0.011823	1.606935
60.809897	723.595329	4.666675	-0.011893	1.614235
61.254690	731.785421	4.671680	-0.011981	1.621465
61.692412	739.998850	4.676685	-0.012068	1.628682
62.247700	748.240217	4.681690	-0.012177	1.635908
62.456052	756.438172	4.686694	-0.012222	1.643016
62.783474	764.640023	4.691699	-0.012288	1.650114
63.396933	772.799738	4.696704	-0.012408	1.657183
63.675340	780.997435	4.701709	-0.012466	1.664210
63.926794	789.223534	4.706714	-0.012518	1.671227
64.362096	797.379885	4.711718	-0.012605	1.678181
64.967007	805.521238	4.716723	-0.012723	1.685116
65.093690	813.757140	4.721728	-0.012752	1.692038
65.562828	821.920783	4.726733	-0.012845	1.698916
66.109312	830.071050	4.731738	-0.012952	1.705766
66.300200	838.293902	4.736742	-0.012994	1.712602
66.613435	846.467843	4.741747	-0.013058	1.719386
66.882579	854.632443	4.746752	-0.013113	1.726130
67.044326	862.835253	4.751757	-0.013149	1.732865
67.521337	870.982210	4.756762	-0.013243	1.739569
67.909400	879.115345	4.761766	-0.013321	1.746224
68.366421	887.292155	4.766771	-0.013412	1.752898
68.644274	895.451572	4.771776	-0.013469	1.759510
68.807847	903.623007	4.776781	-0.013505	1.766092
69.269360	911.785368	4.781786	-0.013597	1.772680
69.561784	919.939548	4.786790	-0.013657	1.779216
69.928929	928.087415	4.791795	-0.013731	1.785732
70.298624	936.283023	4.796800	-0.013805	1.792262
70.627316	944.436519	4.801805	-0.013872	1.798730
70.932718	952.558020	4.806810	-0.013935	1.805147
71.113067	960.715888	4.811814	-0.013974	1.811554
71.436030	968.859376	4.816819	-0.014040	1.817945
71.808966	976.974860	4.821824	-0.014115	1.824298
72.080490	985.123727	4.826829	-0.014171	1.830642
72.602443	993.240960	4.831834	-0.014273	1.836969
72.844136	1001.370379	4.836838	-0.014324	1.843251
73.220526	1009.503860	4.841843	-0.014400	1.849530
73.502284	1017.657343	4.846848	-0.014458	1.855792
73.932429	1025.766049	4.851853	-0.014543	1.862016
74.455868	1033.892794	4.856858	-0.014647	1.868244
74.822827	1042.052433	4.861862	-0.014720	1.874458
75.470788	1050.134044	4.866867	-0.014847	1.880624
75.771242	1058.271332	4.871872	-0.014908	1.886773
75.910325	1066.428255	4.876877	-0.014940	1.892897
76.466656	1074.540031	4.881882	-0.015049	1.899016
76.883919	1082.633381	4.886886	-0.015132	1.905085
77.118162	1090.806574	4.891891	-0.015181	1.911173
77.460182	1098.933939	4.896896	-0.015251	1.917220
77.867489	1107.034790	4.901901	-0.015332	1.923236
78.056260	1115.192855	4.906906	-0.015373	1.929251
78.283834	1123.316078	4.911910	-0.015421	1.935226
78.726983	1131.416141	4.916915	-0.015509	1.941189
79.014591	1139.535457	4.921920	-0.015568	1.947130
79.323362	1147.697569	4.926925	-0.015631	1.953087
79.723354	1155.803798	4.931930	-0.015711	1.958995
80.066789	1163.873317	4.936934	-0.015780	1.964853
80.355652	1172.000820	4.941939	-0.015840	1.970729
80.641105	1180.129590	4.946944	-0.015899	1.976588
80.920793	1188.217339	4.951949	-0.015956	1.982399
81.250885	1196.335832	4.956954	-0.016023	1.988221
81.460636	1204.465071	4.961958	-0.016068	1.994021
82.087592	1212.522486	4.966963	-0.016190	1.999796
82.215865	1220.644700	4.971968	-0.016220	2.005549
82.410222	1228.767043	4.976973	-0.016261	2.011292
82.834593	1236.878773	4.981978	-0.016346	2.017035
83.267088	1244.938928	4.986982	-0.016432	2.022726
83.574509	1253.056264	4.991987	-0.016495	2.028428
83.809728	1261.222158	4.996992	-0.016544	2.034140
83.998746	1269.301894	5.001997	-0.016585	2.039772
84.592328	1277.356672	5.007002	-0.016701	2.045413
84.846268	1285.450733	5.012006	-0.016754	2.051030
85.268371	1293.558911	5.017011	-0.016838	2.056658
85.609227	1301.650122	5.022016	-0.016907	2.062252
85.736885	1309.759146	5.027021	-0.016936	2.067820
86.356842	1317.845550	5.032026	-0.017057	2.073408
86.605192	1325.935017	5.037030	-0.017109	2.078945
86.892900	1334.025822	5.042035	-0.017168	2.084473
87.221440	1342.138409	5.047040	-0.017235	2.090004
87.322455	1350.273179	5.052045	-0.017259	2.095514
87.622863	1358.360227	5.057050	-0.017321	2.100996
87.718635	1366.462471	5.062054	-0.017344	2.106455
88.035583	1374.604890	5.067059	-0.017409	2.111947
88.331039	1382.708792	5.072064	-0.017470	2.117398
88.761360	1390.733340	5.077069	-0.017555	2.122794
89.065077	1398.823643	5.082074	-0.017617	2.128208
89.433440	1406.894665	5.087078	-0.017691	2.133602
89.731575	1414.981619	5.092083	-0.017752	2.138986
89.980584	1423.062397	5.097088	-0.017804	2.144347
90.343223	1431.127651	5.102093	-0.017877	2.149696
90.831620	1439.232400	5.107098	-0.017974	2.155069
90.942074	1447.301576	5.112102	-0.018000	2.160370
91.166486	1455.407642	5.117107	-0.018047	2.165692
91.281893	1463.508147	5.122112	-0.018074	2.170988
91.569399	1471.591099	5.127117	-0.018134	2.176275
91.789150	1479.692723	5.132122	-0.018180	2.181556
91.886987	1487.775454	5.137126	-0.018204	2.186800
92.122844	1495.897562	5.142131	-0.018253	2.192069
92.413667	1503.964711	5.147136	-0.018313	2.197296
92.652336	1512.009319	5.152141	-0.018363	2.202490
93.316171	1520.050195	5.157146	-0.018492	2.207709
93.565640	1528.139875	5.162150	-0.018544	2.212909
93.835291	1536.223177	5.167155	-0.018600	2.218094
94.185713	1544.290956	5.172160	-0.018671	2.223264
94.331076	1552.386368	5.177165	-0.018703	2.228422
94.547098	1560.514673	5.182170	-0.018749	2.233595
94.691635	1568.567232	5.187174	-0.018782	2.238702
95.240332	1576.612821	5.192179	-0.018889	2.243828
95.135493	1584.755176	5.197184	-0.018875	2.248946
95.519801	1592.812346	5.202189	-0.018952	2.254041
96.119547	1600.836892	5.207194	-0.019070	2.259124
96.374053	1608.892642	5.212198	-0.019122	2.264184
96.681400	1616.999353	5.217203	-0.019185	2.269269
96.916878	1625.173586	5.222208	-0.019235	2.274379
97.053903	1633.205153	5.227213	-0.019266	2.279380
97.299044	1641.264755	5.232218	-0.019317	2.284397
97.622226	1649.300674	5.237222	-0.019383	2.289394
98.165221	1657.354771	5.242227	-0.019489	2.294411
98.491758	1665.407154	5.247232	-0.019556	2.299397
98.576073	1673.489393	5.252237	-0.019577	2.304370
98.858230	1681.584731	5.257242	-0.019635	2.309357
99.176939	1689.660077	5.262246	-0.019700	2.314324
99.562125	1697.694514	5.267251	-0.019777	2.319261
99.950961	1705.760471	5.272256	-0.019855	2.324207
99.901914	1713.860890	5.277261	-0.019851	2.329127
100.518506	1721.922868	5.282266	-0.019972	2.334068
100.695868	1729.985116	5.287270	-0.020010	2.338963
100.974870	1738.053957	5.292275	-0.020068	2.343860
100.974818	1746.168094	5.297280	-0.020073	2.348751
101.154998	1754.267496	5.302285	-0.020112	2.353637
101.558555	1762.307867	5.307290	-0.020193	2.358496
101.796898	1770.346436	5.312294	-0.020243	2.363331
101.871413	1778.432595	5.317299	-0.020262	2.368171
102.323260	1786.486171	5.322304	-0.020352	2.373012
102.711900	1794.521688	5.327309	-0.020430	2.377827
102.900690	1802.597413	5.332314	-0.020471	2.382640
103.247537	1810.623636	5.337318	-0.020541	2.387427
103.583146	1818.724749	5.342323	-0.020609	2.392247
103.703918	1826.806035	5.347328	-0.020637	2.397029
103.874549	1834.856603	5.352333	-0.020674	2.401787
104.353965	1842.911366	5.357338	-0.020769	2.406563
104.635796	1850.976517	5.362342	-0.020827	2.411319
104.742597	1859.075159	5.367347	-0.020852	2.416072
105.037308	1867.128042	5.372352	-0.020913	2.420804
105.072324	1875.196988	5.377357	-0.020925	2.425515
105.220459	1883.312581	5.382362	-0.020958	2.430254
105.597009	1891.404298	5.387366	-0.021034	2.434986
106.287074	1899.391247	5.392371	-0.021168	2.439673
106.134931	1907.463549	5.397376	-0.021145	2.444336
106.574505	1915.490192	5.402381	-0.021232	2.449008
107.007646	1923.566350	5.407386	-0.021319	2.453699
107.164034	1931.617976	5.412390	-0.021353	2.458347
107.512345	1939.660116	5.417395	-0.021424	2.462994
107.915369	1947.699365	5.422400	-0.021504	2.467636
108.160982	1955.775364	5.427405	-0.021555	2.472277
108.288643	1963.864568	5.432410	-0.021585	2.476909
108.604033	1971.881310	5.437414	-0.021649	2.481504
108.878812	1979.925532	5.442419	-0.021706	2.486104
109.155543	1988.010706	5.447424	-0.021763	2.490719
109.276711	1996.083811	5.452429	-0.021791	2.495306
109.646628	2004.128120	5.457434	-0.021865	2.499887
109.961279	2012.150319	5.462438	-0.021929	2.504443
110.103023	2020.242854	5.467443	-0.021961	2.509018
110.556212	2028.335723	5.472448	-0.022051	2.513607
110.659261	2036.379669	5.477453	-0.022076	2.518135
110.798505	2044.434361	5.482458	-0.022107	2.522664
111.032425	2052.468061	5.487462	-0.022156	2.527179
111.506168	2060.511892	5.492467	-0.022250	2.531709
111.680707	2068.598556	5.497472	-0.022288	2.536234
111.690325	2076.644780	5.502477	-0.022296	2.540716
112.036002	2084.679595	5.507482	-0.022365	2.545207
112.387478	2092.723303	5.512486	-0.022436	2.549696
112.446571	2100.829515	5.517491	-0.022453	2.554191
112.912150	2108.844309	5.522496	-0.022545	2.558656
113.112003	2116.876732	5.527501	-0.022588	2.563105
113.328474	2124.955446	5.532506	-0.022634	2.567572
113.534984	2133.020946	5.537510	-0.022678	2.572024
113.988670	2141.054067	5.542515	-0.022768	2.576467
114.414604	2149.093432	5.547520	-0.022853	2.580904
114.352363	2157.161076	5.552525	-0.022847	2.585315
114.659558	2165.228768	5.557530	-0.022909	2.589743
115.011936	2173.467810	5.562534	-0.022981	2.594261
115.104052	2181.487948	5.567539	-0.023003	2.598634
115.585203	2189.439787	5.572544	-0.023098	2.602989
115.846072	2197.446209	5.577549	-0.023152	2.607351
116.179543	2205.506494	5.582554	-0.023220	2.611740
116.291356	2213.557801	5.587558	-0.023246	2.616102
116.833281	2221.549047	5.592563	-0.023353	2.620453
116.943245	2229.616066	5.597568	-0.023379	2.624808
117.170785	2237.657061	5.602573	-0.023427	2.629150
117.648275	2245.730677	5.607578	-0.023521	2.633519
117.976020	2253.746720	5.612582	-0.023588	2.637840
118.117133	2261.799063	5.617587	-0.023619	2.642161
118.239827	2269.866358	5.622592	-0.023648	2.646482
118.519040	2277.908701	5.627597	-0.023705	2.650792
118.743036	2286.000683	5.632602	-0.023753	2.655118
118.829669	2294.034096	5.637606	-0.023774	2.659397
119.048435	2302.078506	5.642611	-0.023820	2.663684
119.354332	2310.135416	5.647616	-0.023883	2.667975
119.548664	2318.199579	5.652621	-0.023925	2.672257
119.699825	2326.270218	5.657626	-0.023958	2.676532
120.148102	2334.258034	5.662630	-0.024047	2.680776
120.500310	2342.272184	5.667635	-0.024118	2.685021
120.627820	2350.344798	5.672640	-0.024148	2.689275
120.850305	2358.408110	5.677645	-0.024195	2.693524
121.000989	2366.457784	5.682650	-0.024228	2.697754
121.037135	2374.492185	5.687654	-0.024241	2.701962
121.543913	2382.495191	5.692659	-0.024340	2.706177
121.677970	2390.594568	5.697664	-0.024371	2.710413
121.731340	2398.659391	5.702669	-0.024386	2.714618
122.115998	2406.687572	5.707674	-0.024464	2.718819
122.343432	2414.699032	5.712678	-0.024511	2.722995
122.679405	2422.737113	5.717683	-0.024579	2.727184
122.774400	2430.825457	5.722688	-0.024603	2.731379
123.064165	2438.850608	5.727693	-0.024662	2.735546
123.486835	2446.894209	5.732698	-0.024746	2.739725
123.586836	2454.933355	5.737702	-0.024771	2.743875
123.913686	2462.991940	5.742707	-0.024837	2.748042
124.149618	2471.097994	5.747712	-0.024886	2.752222
124.482799	2479.147831	5.752717	-0.024954	2.756373
124.605639	2487.207277	5.757722	-0.024982	2.760510
124.739129	2495.199468	5.762726	-0.025013	2.764606
124.831546	2503.231038	5.767731	-0.025035	2.768715
125.096250	2511.294268	5.772736	-0.025090	2.772843
125.358169	2519.311106	5.777741	-0.025145	2.776942
125.794232	2527.345452	5.782746	-0.025231	2.781053
125.881924	2535.372178	5.787750	-0.025253	2.785134
126.024435	2543.429014	5.792755	-0.025285	2.789228
126.262985	2551.509472	5.797760	-0.025335	2.793333
126.560219	2559.515443	5.802765	-0.025396	2.797398
126.867499	2567.547544	5.807770	-0.025459	2.801471
127.156031	2575.576943	5.812774	-0.025518	2.805535
127.548265	2583.607451	5.817779	-0.025597	2.809600
127.621288	2591.712007	5.822784	-0.025616	2.813677
127.815709	2599.721057	5.827789	-0.025657	2.817708
128.115636	2607.776980	5.832794	-0.025719	2.821763
128.431808	2615.794735	5.837798	-0.025783	2.825793
128.618394	2623.841421	5.842803	-0.025823	2.829825
128.945838	2631.936228	5.847808	-0.025890	2.833883
129.175391	2639.944871	5.852813	-0.025938	2.837887
129.358045	2647.999798	5.857818	-0.025978	2.841905
129.403581	2656.034629	5.862822	-0.025992	2.845900
129.596277	2664.079862	5.867827	-0.026033	2.849903
129.801925	2672.136948	5.872832	-0.026077	2.853906
130.205965	2680.147723	5.877837	-0.026158	2.857892
130.421710	2688.198077	5.882842	-0.026203	2.861882
130.590259	2696.233439	5.887846	-0.026240	2.865856
130.944546	2704.256035	5.892851	-0.026312	2.869828
131.203929	2712.324077	5.897856	-0.026366	2.873812
131.228376	2720.369975	5.902861	-0.026376	2.877767
131.340760	2728.411412	5.907866	-0.026402	2.881719
131.858808	2736.416824	5.912870	-0.026504	2.885670
132.015621	2744.451986	5.917875	-0.026539	2.889610
132.284325	2752.510075	5.922880	-0.026594	2.893562
132.384719	2760.564066	5.927885	-0.026619	2.897498
132.704078	2768.581112	5.932890	-0.026684	2.901422
132.979592	2776.594777	5.937894	-0.026740	2.905337
133.094335	2784.662212	5.942899	-0.026767	2.909263
133.113598	2792.823227	5.947904	-0.026776	2.913225
133.391009	2800.803915	5.952909	-0.026834	2.917108
133.833290	2808.828295	5.957914	-0.026921	2.921016
133.967748	2816.813357	5.962918	-0.026952	2.924883
134.123157	2824.852725	5.967923	-0.026986	2.928772
134.231225	2832.907389	5.972928	-0.027012	2.932660
134.500446	2840.933840	5.977933	-0.027068	2.936539
135.060854	2848.940041	5.982938	-0.027178	2.940418
135.104031	2856.956660	5.987942	-0.027191	2.944269
135.113532	2865.036317	5.992947	-0.027198	2.948144
135.572888	2873.081225	5.997952	-0.027290	2.952021
135.839522	2881.128374	6.002957	-0.027345	2.955883
135.981609	2889.156452	6.007962	-0.027377	2.959725
136.402690	2897.130324	6.012966	-0.027461	2.963551
136.773986	2905.181060	6.017971	-0.027535	2.967405
136.738798	2913.300482	6.022976	-0.027534	2.971266
136.906110	2921.329895	6.027981	-0.027571	2.975090
137.368373	2929.341528	6.032986	-0.027662	2.978916
137.586949	2937.350137	6.037990	-0.027709	2.982722
137.669903	2945.420491	6.042995	-0.027730	2.986546
137.837129	2953.467178	6.048000	-0.027766	2.990359
138.030008	2961.534744	6.053005	-0.027808	2.994177
138.411852	2969.539718	6.058010	-0.027884	2.997971
138.410596	2977.560344	6.063014	-0.027890	3.001748
138.563974	2985.588725	6.068019	-0.027924	3.005531
138.967922	2993.580991	6.073024	-0.028004	3.009306
138.931555	3001.681700	6.078029	-0.028003	3.013104
139.375617	3009.706246	6.083034	-0.028091	3.016886
139.373629	3017.752397	6.088038	-0.028097	3.020651
139.482038	3025.750941	6.093043	-0.028122	3.024394
139.847171	3033.799620	6.098048	-0.028196	3.028169
140.102559	3041.833775	6.103053	-0.028249	3.031927
140.197608	3049.932936	6.108058	-0.028272	3.035703
140.166073	3057.921681	6.113062	-0.028272	3.039417
140.581012	3065.928465	6.118067	-0.028354	3.043156
140.775115	3073.979577	6.123072	-0.028396	3.046900
140.910081	3082.006342	6.128077	-0.028427	3.050625
141.100227	3090.069047	6.133082	-0.028468	3.054365
141.309927	3098.095124	6.138086	-0.028512	3.058085
141.494124	3106.143176	6.143091	-0.028552	3.061809
141.694722	3114.187256	6.148096	-0.028595	3.065527
141.924082	3122.198931	6.153101	-0.028643	3.069227
142.258348	3130.298004	6.158106	-0.028711	3.072968
142.567407	3138.323326	6.163110	-0.028774	3.076669
142.749417	3146.311462	6.168115	-0.028813	3.080343
143.079759	3154.307837	6.173120	-0.028880	3.084023
143.202466	3162.356779	6.178125	-0.028909	3.087713
143.659988	3170.390505	6.183130	-0.029000	3.091407
143.878866	3178.425287	6.188134	-0.029046	3.095086
143.896505	3186.451627	6.193139	-0.029055	3.098747
144.153279	3194.501194	6.198144	-0.029108	3.102426
144.384359	3202.519087	6.203149	-0.029157	3.106085
144.441085	3210.560552	6.208154	-0.029173	3.109742
144.499276	3218.625137	6.213158	-0.029189	3.113405
144.849381	3226.622648	6.218163	-0.029260	3.117047
145.265638	3234.634850	6.223168	-0.029343	3.120694
145.344277	3242.643168	6.228173	-0.029363	3.124320
145.617359	3250.700360	6.233178	-0.029419	3.127972
146.000310	3258.741032	6.238182	-0.029496	3.131618
146.081613	3266.800226	6.243187	-0.029517	3.135254
146.201473	3274.820624	6.248192	-0.029545	3.138870
146.221199	3282.864343	6.253197	-0.029554	3.142488
146.535522	3290.894035	6.258202	-0.029618	3.146109
146.902445	3298.899451	6.263206	-0.029692	3.149717
146.904449	3307.006329	6.268211	-0.029698	3.153350
147.078176	3315.022087	6.273216	-0.029735	3.156945
147.155498	3323.025013	6.278221	-0.029755	3.160527
147.364828	3331.025650	6.283226	-0.029800	3.164109
147.571262	3339.071461	6.288230	-0.029844	3.167707
147.732769	3347.101428	6.293235	-0.029879	3.171292
147.996907	3355.158043	6.298240	-0.029934	3.174889
148.239096	3363.160701	6.303245	-0.029985	3.178458
148.347957	3371.213427	6.308250	-0.030010	3.182038
148.423902	3379.224215	6.313254	-0.030030	3.185595
148.620449	3387.265597	6.318259	-0.030072	3.189166
149.082298	3395.339468	6.323264	-0.030164	3.192759
149.208184	3403.359291	6.328269	-0.030193	3.196309
149.483142	3411.371096	6.333274	-0.030249	3.199859
149.907929	3419.363557	6.338278	-0.030334	3.203402
150.191428	3427.382721	6.343283	-0.030392	3.206947
150.371679	3435.435569	6.348288	-0.030431	3.210499
150.248125	3443.487005	6.353293	-0.030414	3.214033
150.626867	3451.521312	6.358298	-0.030490	3.217577
150.629784	3459.565790	6.363302	-0.030496	3.221106
150.972099	3467.535955	6.368307	-0.030565	3.224612
151.433597	3475.571625	6.373312	-0.030657	3.228148
151.507357	3483.645388	6.378317	-0.030676	3.231681
151.915969	3491.723306	6.383322	-0.030758	3.235225
152.189851	3499.716837	6.388326	-0.030814	3.238723
152.240243	3507.737733	6.393331	-0.030829	3.242221
152.550979	3515.763316	6.398336	-0.030892	3.245727
152.733196	3523.752136	6.403341	-0.030932	3.249208
153.029783	3531.815310	6.408346	-0.030992	3.252722
153.167299	3539.865990	6.413350	-0.031024	3.256220
153.519599	3547.831455	6.418355	-0.031095	3.259687
153.936491	3555.875420	6.423360	-0.031178	3.263186
153.960170	3563.923719	6.428365	-0.031188	3.266668
154.043275	3571.962190	6.433370	-0.031209	3.270144
154.183244	3580.034488	6.438374	-0.031240	3.273633
154.413315	3588.044976	6.443379	-0.031289	3.277095
154.873268	3596.057733	6.448384	-0.031380	3.280564
154.767095	3604.072298	6.453389	-0.031366	3.284007
155.130604	3612.121183	6.458394	-0.031439	3.287480
155.225122	3620.154955	6.463398	-0.031462	3.290932
155.468229	3628.168570	6.468403	-0.031513	3.294378
155.915995	3636.205169	6.473408	-0.031602	3.297838
155.825875	3644.255476	6.478413	-0.031590	3.301279
156.073086	3652.238002	6.483418	-0.031642	3.304701
156.245973	3660.280169	6.488422	-0.031680	3.308142
156.427733	3668.324886	6.493427	-0.031719	3.311580
156.744629	3676.382938	6.498432	-0.031783	3.315026
156.780571	3684.381932	6.503437	-0.031796	3.318433
157.136394	3692.399864	6.508442	-0.031867	3.321855
157.310356	3700.381967	6.513446	-0.031905	3.325253
157.459141	3708.409132	6.518451	-0.031939	3.328665
157.862674	3716.448798	6.523456	-0.032019	3.332088
158.154440	3724.493438	6.528461	-0.032079	3.335506
158.210691	3732.536025	6.533466	-0.032095	3.338910
158.325554	3740.569186	6.538470	-0.032122	3.342310
158.674214	3748.582869	6.543475	-0.032192	3.345706
158.865381	3756.622970	6.548480	-0.032233	3.349104
158.801247	3764.685270	6.553485	-0.032227	3.352498
159.144731	3772.733146	6.558490	-0.032297	3.355898
159.422434	3780.690274	6.563494	-0.032354	3.359254
159.643528	3788.705725	6.568499	-0.032400	3.362629
159.791717	3796.775789	6.573504	-0.032434	3.366021
159.911571	3804.771550	6.578509	-0.032461	3.369377
160.136754	3812.849895	6.583514	-0.032509	3.372768
160.385512	3820.895654	6.588518	-0.032561	3.376143
160.380180	3828.882987	6.593523	-0.032565	3.379481
160.605941	3836.923718	6.598528	-0.032613	3.382846
160.673207	3844.932807	6.603533	-0.032631	3.386189
161.004799	3852.961277	6.608538	-0.032698	3.389546
161.119429	3861.087422	6.613542	-0.032725	3.392933
161.235947	3869.093150	6.618547	-0.032752	3.396266
161.702235	3877.069977	6.623552	-0.032844	3.399596
162.016100	3885.028461	6.628557	-0.032908	3.402910
162.224155	3893.082783	6.633562	-0.032953	3.406257
162.250801	3901.118000	6.638566	-0.032963	3.409587
162.521419	3909.115928	6.643571	-0.033019	3.412906
162.831892	3917.175143	6.648576	-0.033082	3.416248
162.808813	3925.169376	6.653581	-0.033084	3.419549
163.190597	3933.168995	6.658586	-0.033160	3.422863
163.301509	3941.234445	6.663590	-0.033186	3.426191
163.330571	3949.260658	6.668595	-0.033197	3.429497
163.696505	3957.283009	6.673600	-0.033271	3.432810
163.719377	3965.363340	6.678605	-0.033281	3.436132
164.055946	3973.328584	6.683610	-0.033349	3.439414
164.131775	3981.379898	6.688614	-0.033368	3.442719
164.306114	3989.392898	6.693619	-0.033406	3.446008
164.510820	3997.427208	6.698624	-0.033450	3.449305
164.660667	4005.498933	6.703629	-0.033484	3.452611
164.936951	4013.524729	6.708634	-0.033540	3.455900
164.939754	4021.542008	6.713638	-0.033546	3.459173
165.009340	4029.573027	6.718643	-0.033565	3.462451
165.471165	4037.578824	6.723648	-0.033656	3.465728
165.735323	4045.595899	6.728653	-0.033711	3.469000
165.963735	4053.664990	6.733658	-0.033759	3.472289
166.186249	4061.693882	6.738662	-0.033806	3.475559
166.295187	4069.660944	6.743667	-0.033832	3.478796
166.526736	4077.724394	6.748672	-0.033881	3.482074
166.604462	4085.698195	6.753677	-0.033901	3.485307
166.723485	4093.766484	6.758682	-0.033928	3.488576
167.067391	4101.798525	6.763686	-0.033998	3.491835
167.307388	4109.787602	6.768691	-0.034048	3.495071
167.251997	4117.862942	6.773696	-0.034043	3.498329
167.500499	4125.832314	6.778701	-0.034095	3.501550
167.685253	4133.852079	6.783706	-0.034135	3.504787
167.734782	4141.895246	6.788710	-0.034150	3.508026
167.952010	4149.915070	6.793715	-0.034196	3.511258
168.504195	4157.950036	6.798720	-0.034304	3.514503
168.377175	4165.974032	6.803725	-0.034286	3.517720
168.612927	4173.993115	6.808730	-0.034335	3.520943
168.924958	4181.992785	6.813734	-0.034399	3.524158
169.016400	4190.040910	6.818739	-0.034421	3.527383
169.260906	4198.092624	6.823744	-0.034472	3.530610
169.478596	4206.103829	6.828749	-0.034518	3.533818
169.829132	4214.161669	6.833754	-0.034589	3.537045
169.788667	4222.186825	6.838758	-0.034587	3.540244
169.775011	4230.194481	6.843763	-0.034590	3.543435
170.092365	4238.219039	6.848768	-0.034655	3.546639
170.226702	4246.249784	6.853773	-0.034685	3.549837
170.323944	4254.366065	6.858778	-0.034709	3.553065
170.631109	4262.404921	6.863782	-0.034772	3.556266
170.872109	4270.324578	6.868787	-0.034822	3.559414
171.139224	4278.357405	6.873792	-0.034877	3.562606
170.956872	4286.377910	6.878797	-0.034849	3.565776
171.399972	4294.359401	6.883802	-0.034937	3.568946
171.734971	4302.413831	6.888806	-0.035005	3.572140
171.767147	4310.425840	6.893811	-0.035016	3.575304
172.086504	4318.461982	6.898816	-0.035081	3.578484
172.235578	4326.470294	6.903821	-0.035114	3.581645
172.554284	4334.478976	6.908826	-0.035179	3.584808
172.828574	4342.520330	6.913830	-0.035236	3.587980
172.957771	4350.556384	6.918835	-0.035265	3.591143
173.223975	4358.584142	6.923840	-0.035321	3.594304
173.359195	4366.560863	6.928845	-0.035351	3.597438
173.744010	4374.592825	6.933850	-0.035428	3.600598
173.771930	4382.600944	6.938854	-0.035439	3.603736
173.882334	4390.646888	6.943859	-0.035465	3.606888
174.266828	4398.684424	6.948864	-0.035542	3.610042
174.263691	4406.740681	6.953869	-0.035547	3.613190
174.440069	4414.773667	6.958874	-0.035586	3.616331
174.701028	4422.720469	6.963878	-0.035640	3.619437
175.156393	4430.756725	6.968883	-0.035730	3.622581
175.230992	4438.822880	6.973888	-0.035749	3.625724
175.351476	4446.806954	6.978893	-0.035777	3.628833
175.604302	4454.914065	6.983898	-0.035830	3.631991
175.683273	4462.973693	6.988902	-0.035850	3.635123
175.807540	4470.921254	6.993907	-0.035879	3.638210
176.161744	4478.986210	6.998912	-0.035950	3.641346
176.122239	4486.924175	7.003917	-0.035948	3.644420
176.364265	4494.958413	7.008922	-0.035999	3.647536
176.412901	4503.020983	7.013926	-0.036014	3.650655
176.482395	4511.048628	7.018931	-0.036032	3.653758
176.656598	4519.111596	7.023936	-0.036070	3.656875
176.840304	4527.071556	7.028941	-0.036110	3.659950
176.907315	4535.119971	7.033946	-0.036128	3.663053
176.998967	4543.167904	7.038950	-0.036150	3.666154
177.004863	4551.165968	7.043955	-0.036157	3.669231
177.480669	4559.185474	7.048960	-0.036251	3.672326
177.646511	4567.215669	7.053965	-0.036287	3.675414
177.818055	4575.226272	7.058970	-0.036325	3.678492
178.112957	4583.269662	7.063974	-0.036385	3.681584
178.208272	4591.221517	7.068979	-0.036408	3.684633
178.654391	4599.275897	7.073984	-0.036497	3.687727
178.646533	4607.300275	7.078989	-0.036501	3.690795
178.976035	4615.334449	7.083994	-0.036568	3.693874
179.182913	4623.388442	7.088998	-0.036612	3.696954
179.403335	4631.359940	7.094003	-0.036659	3.700000
179.534297	4639.393120	7.099008	-0.036688	3.703065
179.487909	4647.433906	7.104013	-0.036685	3.706127
179.768957	4655.434630	7.109018	-0.036743	3.709178
179.902953	4663.506629	7.114022	-0.036774	3.712250
180.125287	4671.560774	7.119027	-0.036821	3.715316
180.331253	4679.549497	7.124032	-0.036864	3.718353
180.363895	4687.551848	7.129037	-0.036876	3.721389
180.720592	4695.526026	7.134042	-0.036948	3.724419
180.878941	4703.537653	7.139046	-0.036983	3.727457
180.865220	4711.571780	7.144051	-0.036986	3.730496
181.303303	4719.631760	7.149056	-0.037073	3.733553
181.448989	4727.653342	7.154061	-0.037106	3.736587
181.454607	4735.659714	7.159066	-0.037112	3.739609
181.557870	4743.676382	7.164070	-0.037137	3.742634
181.657659	4751.660019	7.169075	-0.037161	3.745645
181.981520	4759.711646	7.174080	-0.037227	3.748684
181.945527	4767.754142	7.179085	-0.037226	3.751708
182.285585	4775.818864	7.184090	-0.037294	3.754747
182.427770	4783.826827	7.189094	-0.037326	3.757758
182.660521	4791.819892	7.194099	-0.037375	3.760763
182.845751	4799.819877	7.199104	-0.037415	3.763767
182.911908	4807.857807	7.204109	-0.037433	3.766780
183.090885	4815.900331	7.209114	-0.037472	3.769795
183.280218	4823.944575	7.214118	-0.037513	3.772809
183.550303	4831.963706	7.219123	-0.037568	3.775812
183.511539	4839.992957	7.224128	-0.037567	3.778810
183.566993	4848.016205	7.229133	-0.037583	3.781805
183.987702	4856.006324	7.234138	-0.037666	3.784794
184.263188	4864.031761	7.239142	-0.037723	3.787790
184.248122	4872.053326	7.244147	-0.037726	3.790776
184.462043	4880.153245	7.249152	-0.037771	3.793793
184.730384	4888.127924	7.254157	-0.037827	3.796763
184.803047	4896.081003	7.259162	-0.037846	3.799719
185.002290	4904.138064	7.264166	-0.037888	3.802713
185.180554	4912.110991	7.269171	-0.037927	3.805673
185.291056	4920.143908	7.274176	-0.037953	3.808652
185.298105	4928.220414	7.279181	-0.037960	3.811642
185.550135	4936.225720	7.284186	-0.038012	3.814609
185.616507	4944.239675	7.289190	-0.038030	3.817573
185.767547	4952.202582	7.294195	-0.038064	3.820517
186.159104	4960.243344	7.299200	-0.038142	3.823493
186.177050	4968.286555	7.304205	-0.038151	3.826460
186.605400	4976.264268	7.309210	-0.038236	3.829408
186.829239	4984.371086	7.314214	-0.038284	3.832398
186.884917	4992.371636	7.319219	-0.038300	3.835343
186.918164	5000.403423	7.324224	-0.038311	3.838296
187.047201	5008.413915	7.329229	-0.038341	3.841241
187.220433	5016.376234	7.334234	-0.038379	3.844168
187.479132	5024.414855	7.339238	-0.038432	3.847121
187.648558	5032.420437	7.344243	-0.038469	3.850059
187.796817	5040.522939	7.349248	-0.038502	3.853029
188.018432	5048.497972	7.354253	-0.038549	3.855952
188.187693	5056.535859	7.359258	-0.038586	3.858894
188.335569	5064.579428	7.364262	-0.038619	3.861836
188.294336	5072.580535	7.369267	-0.038617	3.864756
188.808429	5080.626715	7.374272	-0.038718	3.867702
188.795430	5088.645384	7.379277	-0.038721	3.870625
189.134782	5096.867093	7.384282	-0.038790	3.873626
189.138032	5104.902392	7.389286	-0.038796	3.876551
189.182098	5112.769826	7.394291	-0.038810	3.879413
189.491117	5120.776702	7.399296	-0.038873	3.882329
189.512457	5128.744904	7.404301	-0.038882	3.885223
189.760345	5136.728523	7.409306	-0.038934	3.888125
189.806182	5144.771139	7.414310	-0.038948	3.891043
190.279715	5152.807565	7.419315	-0.039042	3.893963
190.581440	5160.854967	7.424320	-0.039104	3.896883
190.611136	5168.812310	7.429325	-0.039115	3.899762
190.808281	5176.843692	7.434330	-0.039157	3.902669
191.141879	5184.890479	7.439334	-0.039224	3.905583
191.075637	5192.866393	7.444339	-0.039218	3.908460
191.348247	5200.927632	7.449344	-0.039274	3.911373
191.763522	5208.946936	7.454349	-0.039357	3.914271
191.749111	5216.979661	7.459354	-0.039360	3.917164
192.062009	5224.948669	7.464358	-0.039423	3.920038
191.929212	5232.968928	7.469363	-0.039404	3.922920
192.337369	5240.993683	7.474368	-0.039486	3.925811
192.397922	5248.993386	7.479373	-0.039502	3.928685
192.626695	5257.056666	7.484378	-0.039551	3.931583
192.985564	5265.083769	7.489382	-0.039623	3.934467
193.010736	5273.076052	7.494387	-0.039633	3.937332
193.313071	5281.095283	7.499392	-0.039695	3.940208
193.338750	5289.115009	7.504397	-0.039705	3.943078
193.634605	5297.114164	7.509402	-0.039766	3.945943
193.612288	5305.145391	7.514406	-0.039767	3.948812
193.783246	5313.180870	7.519411	-0.039804	3.951683
194.302765	5321.226296	7.524416	-0.039907	3.954562
194.156107	5329.243573	7.529421	-0.039885	3.957418
194.369062	5337.226399	7.534426	-0.039930	3.960265
194.441449	5345.250792	7.539430	-0.039949	3.963123
194.545780	5353.239094	7.544435	-0.039974	3.965966
194.835215	5361.276178	7.549440	-0.040033	3.968828
194.880068	5369.307969	7.554445	-0.040047	3.971681
195.163552	5377.350094	7.559450	-0.040106	3.974540
195.129334	5385.398161	7.564454	-0.040105	3.977394
195.266914	5393.359331	7.569459	-0.040136	3.980218
195.518635	5401.381726	7.574464	-0.040188	3.983063
195.672054	5409.402198	7.579469	-0.040222	3.985904
195.689703	5417.444481	7.584474	-0.040231	3.988749
195.891553	5425.505217	7.589478	-0.040274	3.991601
196.110224	5433.494096	7.594483	-0.040320	3.994425
196.294581	5441.541634	7.599488	-0.040360	3.997268
196.366672	5449.504459	7.604493	-0.040379	4.000078
196.663399	5457.535387	7.609498	-0.040440	4.002912
196.678456	5465.573356	7.614502	-0.040448	4.005743
196.773632	5473.576138	7.619507	-0.040471	4.008561
197.253702	5481.649934	7.624512	-0.040566	4.011407
197.221654	5489.661890	7.629517	-0.040566	4.014222
197.458184	5497.687088	7.634522	-0.040615	4.017044
197.537771	5505.693832	7.639526	-0.040636	4.019854
197.713927	5513.696621	7.644531	-0.040674	4.022663
197.901688	5521.729533	7.649536	-0.040715	4.025481
198.186533	5529.734484	7.654541	-0.040773	4.028288
198.225883	5537.804023	7.659546	-0.040786	4.031112
198.319342	5545.923349	7.664550	-0.040809	4.033953
198.271865	5553.897206	7.669555	-0.040806	4.036738
198.594238	5561.846379	7.674560	-0.040871	4.039519
198.717158	5569.826696	7.679565	-0.040899	4.042305
198.909125	5577.810538	7.684570	-0.040941	4.045092
199.022118	5585.857991	7.689574	-0.040967	4.047898
199.195249	5593.878950	7.694579	-0.041005	4.050693
199.230982	5601.948990	7.699584	-0.041017	4.053502
199.342047	5609.955938	7.704589	-0.041043	4.056287
199.621952	5617.897616	7.709594	-0.041101	4.059051
199.801929	5625.961389	7.714598	-0.041140	4.061854
199.968238	5633.917973	7.719603	-0.041176	4.064617
200.305982	5641.966694	7.724608	-0.041245	4.067413
200.530410	5649.995077	7.729613	-0.041292	4.070198
200.537074	5658.024369	7.734618	-0.041299	4.072978
200.800070	5666.074078	7.739622	-0.041353	4.075767
201.061018	5674.042800	7.744627	-0.041407	4.078527
201.081981	5682.126044	7.749632	-0.041417	4.081320
201.212939	5690.063053	7.754637	-0.041447	4.084063
201.500611	5698.098801	7.759642	-0.041506	4.086840
201.725232	5706.131761	7.764646	-0.041553	4.089613
201.497038	5714.173530	7.769651	-0.041516	4.092381
201.799521	5722.199046	7.774656	-0.041578	4.095149
202.329478	5730.158679	7.779661	-0.041682	4.097896
202.337303	5738.215787	7.784666	-0.041689	4.100667
202.317238	5746.232175	7.789670	-0.041691	4.103422
202.503510	5754.211506	7.794675	-0.041731	4.106165
202.827547	5762.276550	7.799680	-0.041797	4.108937
202.807232	5770.311958	7.804685	-0.041799	4.111693
203.087903	5778.334134	7.809690	-0.041856	4.114446
203.217452	5786.396645	7.814694	-0.041886	4.117209
203.394384	5794.342434	7.819699	-0.041925	4.119932
203.734554	5802.378807	7.824704	-0.041993	4.122685
203.863550	5810.352659	7.829709	-0.042023	4.125412
203.897360	5818.395678	7.834714	-0.042035	4.128160
204.135545	5826.453089	7.839718	-0.042085	4.130914
204.322032	5834.475748	7.844723	-0.042125	4.133653
204.538995	5842.533861	7.849728	-0.042171	4.136403
204.197353	5850.502903	7.854733	-0.042113	4.139114
204.474338	5858.515488	7.859738	-0.042170	4.141845
204.873900	5866.507102	7.864742	-0.042250	4.144569
204.700127	5874.531743	7.869747	-0.042223	4.147296
205.070717	5882.574649	7.874752	-0.042297	4.150033
205.330814	5890.591938	7.879757	-0.042351	4.152758
205.607970	5898.637945	7.884762	-0.042408	4.155492
205.744060	5906.620570	7.889766	-0.042439	4.158201
205.858436	5914.654364	7.894771	-0.042466	4.160925
206.103295	5922.646604	7.899776	-0.042517	4.163634
206.119804	5930.699895	7.904781	-0.042526	4.166360
206.281641	5938.669544	7.909786	-0.042561	4.169057
206.476882	5946.728311	7.914790	-0.042603	4.171784
206.683919	5954.732872	7.919795	-0.042647	4.174490
206.559361	5962.775925	7.924800	-0.042630	4.177203
206.881090	5970.766860	7.929805	-0.042695	4.179903
206.962799	5978.777455	7.934810	-0.042716	4.182604
206.965641	5986.791206	7.939814	-0.042722	4.185304
207.337640	5994.805601	7.944819	-0.042796	4.188006
207.675220	6002.841294	7.949824	-0.042865	4.190714
207.732916	6010.946087	7.954829	-0.042881	4.193440
207.634512	6019.001669	7.959834	-0.042868	4.196146
208.132803	6026.891964	7.964838	-0.042967	4.198800
208.150119	6034.946819	7.969843	-0.042975	4.201504
208.323253	6042.869781	7.974848	-0.043013	4.204163
208.369547	6050.894020	7.979853	-0.043027	4.206853
208.543446	6058.912960	7.984858	-0.043065	4.209540
208.598901	6066.977121	7.989862	-0.043081	4.212240
208.731135	6074.975997	7.994867	-0.043111	4.214918
208.897129	6083.037852	7.999872	-0.043147	4.217614
208.894041	6090.994113	8.004877	-0.043152	4.220272
208.859904	6099.018994	8.009882	-0.043152	4.222951
209.098027	6107.026847	8.014886	-0.043201	4.225626
209.359713	6115.054168	8.019891	-0.043256	4.228305
209.357966	6123.076604	8.024896	-0.043261	4.230978
209.598635	6131.128015	8.029901	-0.043311	4.233662
209.916421	6139.159893	8.034906	-0.043376	4.236338
209.976783	6147.124564	8.039910	-0.043393	4.238988
209.966363	6155.184586	8.044915	-0.043396	4.241667
210.335526	6163.148706	8.049920	-0.043470	4.244316
210.346661	6171.188235	8.054925	-0.043478	4.246985
210.367084	6179.178917	8.059930	-0.043487	4.249636
210.760597	6187.251861	8.064934	-0.043566	4.252316
210.932245	6195.240037	8.069939	-0.043603	4.254965
211.078812	6203.320721	8.074944	-0.043636	4.257642
211.184158	6211.269894	8.079949	-0.043661	4.260273
211.236716	6219.293446	8.084954	-0.043677	4.262927
211.576011	6227.310576	8.089958	-0.043745	4.265580
211.602781	6235.343979	8.094963	-0.043756	4.268234
211.838478	6243.393922	8.099968	-0.043805	4.270893
212.139352	6251.482309	8.104973	-0.043867	4.273564
212.269462	6259.496962	8.109978	-0.043897	4.276207
212.470954	6267.461714	8.114982	-0.043940	4.278833
212.269290	6275.468319	8.119987	-0.043908	4.281468
212.313091	6283.441283	8.124992	-0.043921	4.284092
212.473376	6291.479850	8.129997	-0.043957	4.286737
212.787894	6299.502495	8.135002	-0.044021	4.289376
212.897305	6307.555271	8.140006	-0.044047	4.292022
213.162173	6315.541695	8.145011	-0.044101	4.294646
213.420087	6323.583742	8.150016	-0.044155	4.297286
213.544471	6331.550257	8.155021	-0.044184	4.299899
213.550545	6339.583613	8.160026	-0.044190	4.302531
213.722864	6347.612214	8.165030	-0.044228	4.305162
213.922437	6355.593625	8.170035	-0.044270	4.307775
213.788326	6363.686150	8.175040	-0.044251	4.310421
213.790563	6371.715458	8.180045	-0.044257	4.313045
214.082878	6379.681788	8.185050	-0.044317	4.315649
214.189512	6387.682173	8.190054	-0.044342	4.318262
214.276955	6395.708949	8.195059	-0.044364	4.320881
214.556184	6403.694185	8.200064	-0.044421	4.323487
214.789880	6411.754378	8.205069	-0.044471	4.326115
214.806190	6419.707379	8.210074	-0.044479	4.328705
215.062694	6427.785603	8.215078	-0.044532	4.331336
215.321874	6435.772776	8.220083	-0.044586	4.333935
215.435288	6443.849655	8.225088	-0.044613	4.336562
215.512333	6451.763065	8.230093	-0.044633	4.339133
215.775192	6459.836960	8.235098	-0.044687	4.341756
215.749233	6467.845857	8.240102	-0.044688	4.344355
215.810400	6475.872186	8.245107	-0.044705	4.346958
216.139114	6483.888232	8.250112	-0.044771	4.349558
216.340758	6491.966759	8.255117	-0.044814	4.352175
216.079499	6500.023861	8.260122	-0.044771	4.354782
216.484129	6508.027043	8.265126	-0.044852	4.357373
216.699245	6515.931678	8.270131	-0.044898	4.359930
216.768681	6523.960847	8.275136	-0.044916	4.362525
216.873492	6531.950627	8.280141	-0.044941	4.365106
217.180471	6539.949053	8.285146	-0.045004	4.367689
217.203517	6548.006144	8.290150	-0.045014	4.370287
217.267897	6556.027550	8.295155	-0.045031	4.372873
217.618230	6564.087202	8.300160	-0.045102	4.375472
217.529003	6572.088095	8.305165	-0.045091	4.378047
217.705274	6580.065547	8.310170	-0.045129	4.380615
218.087720	6588.081923	8.315174	-0.045206	4.383195
218.188845	6596.091672	8.320179	-0.045230	4.385770
218.181933	6604.122663	8.325184	-0.045234	4.388349
218.236942	6612.171900	8.330189	-0.045250	4.390933
218.497495	6620.178564	8.335194	-0.045304	4.393503
218.650778	6628.226920	8.340198	-0.045338	4.396085
218.714195	6636.156837	8.345203	-0.045355	4.398626
219.176014	6644.220297	8.350208	-0.045447	4.401211
219.148894	6652.186466	8.355213	-0.045447	4.403760
219.034392	6660.245562	8.360218	-0.045432	4.406337
219.460459	6668.261586	8.365222	-0.045516	4.408902
219.425066	6676.293683	8.370227	-0.045515	4.411468
219.467584	6684.303800	8.375232	-0.045529	4.414026
219.599739	6692.332861	8.380237	-0.045559	4.416589
219.831825	6700.314202	8.385242	-0.045608	4.419135
220.026735	6708.392905	8.390246	-0.045649	4.421711
220.082124	6716.355940	8.395251	-0.045665	4.424248
220.302728	6724.429049	8.400256	-0.045712	4.426819
220.472925	6732.420326	8.405261	-0.045749	4.429363
220.524696	6740.436625	8.410266	-0.045764	4.431912
220.985284	6748.522551	8.415270	-0.045855	4.434484
221.208499	6756.523262	8.420275	-0.045902	4.437026
221.237159	6764.495910	8.425280	-0.045913	4.439557
221.351467	6772.519217	8.430285	-0.045940	4.442103
221.314864	6780.462521	8.435290	-0.045939	4.444622
221.444974	6788.537229	8.440294	-0.045969	4.447181
221.682576	6796.521586	8.445299	-0.046018	4.449711
221.996151	6804.619134	8.450304	-0.046082	4.452276
222.019860	6812.606659	8.455309	-0.046092	4.454803
222.406786	6820.608080	8.460314	-0.046170	4.457334
222.729429	6828.659466	8.465318	-0.046235	4.459879
222.604022	6836.623047	8.470323	-0.046217	4.462394
222.886552	6844.630804	8.475328	-0.046275	4.464922
223.039324	6852.690261	8.480333	-0.046309	4.467465
223.252929	6860.659584	8.485338	-0.046355	4.469978
223.638686	6868.740584	8.490342	-0.046432	4.472526
223.584038	6876.749871	8.495347	-0.046427	4.475048
223.575189	6884.750269	8.500352	-0.046431	4.477566
223.855520	6892.697505	8.505357	-0.046489	4.480066
224.011310	6900.733047	8.510362	-0.046523	4.482593
224.185203	6908.775989	8.515366	-0.046561	4.485121
224.216204	6916.798124	8.520371	-0.046573	4.487640
224.273981	6924.812584	8.525376	-0.046589	4.490155
224.335685	6932.865383	8.530381	-0.046606	4.492681
224.508156	6940.843002	8.535386	-0.046644	4.495183
224.689249	6948.909786	8.540390	-0.046683	4.497710
224.853640	6956.875623	8.545395	-0.046719	4.500205
225.216952	6964.857166	8.550400	-0.046792	4.502704
225.311738	6972.851607	8.555405	-0.046815	4.505205
225.323458	6980.926164	8.560410	-0.046823	4.507729
225.530130	6988.937677	8.565415	-0.046867	4.510232
225.675253	6997.019236	8.570419	-0.046899	4.512756
225.969016	7005.051180	8.575424	-0.046960	4.515264
225.808914	7013.017102	8.580429	-0.046935	4.517748
225.966881	7020.961934	8.585434	-0.046970	4.520225
226.188434	7029.010965	8.590439	-0.047017	4.522733
226.210842	7036.980725	8.595443	-0.047027	4.525215
226.371809	7045.034198	8.600448	-0.047062	4.527721
226.528235	7052.992837	8.605453	-0.047097	4.530197
226.746311	7061.077053	8.610458	-0.047143	4.532711
226.798536	7069.135738	8.615463	-0.047158	4.535214
226.923080	7077.108956	8.620467	-0.047187	4.537690
227.104081	7085.104363	8.625472	-0.047226	4.540172
227.283122	7093.106249	8.630477	-0.047265	4.542654
227.393099	7101.117003	8.635482	-0.047291	4.545138
227.799570	7109.177977	8.640487	-0.047372	4.547636
227.806177	7117.148797	8.645491	-0.047379	4.550104
227.921836	7125.235417	8.650496	-0.047406	4.552607
227.996208	7133.254048	8.655501	-0.047425	4.555088
228.040656	7141.221666	8.660506	-0.047439	4.557551
228.139686	7149.201466	8.665511	-0.047463	4.560017
228.330307	7157.225700	8.670515	-0.047504	4.562495
228.644609	7165.242758	8.675520	-0.047568	4.564970
228.705362	7173.297653	8.680525	-0.047585	4.567455
228.536032	7181.272708	8.685530	-0.047559	4.569913
228.944532	7189.345303	8.690535	-0.047640	4.572401
228.949457	7197.347703	8.695539	-0.047647	4.574866
229.144784	7205.389367	8.700544	-0.047689	4.577341
229.240557	7213.394128	8.705549	-0.047712	4.579804
229.439234	7221.407037	8.710554	-0.047754	4.582268
229.554475	7229.403207	8.715559	-0.047781	4.584725
229.644800	7237.437328	8.720563	-0.047804	4.587193
229.834732	7245.456288	8.725568	-0.047845	4.589654
229.945757	7253.519477	8.730573	-0.047871	4.592128
229.989956	7261.520979	8.735578	-0.047885	4.594582
230.427337	7269.567992	8.740583	-0.047971	4.597048
230.312592	7277.479504	8.745587	-0.047956	4.599471
230.465856	7285.570317	8.750592	-0.047990	4.601948
230.688233	7293.496077	8.755597	-0.048036	4.604374
230.760624	7301.556919	8.760602	-0.048056	4.606839
230.844194	7309.559785	8.765607	-0.048077	4.609285
230.882685	7317.612957	8.770611	-0.048089	4.611745
231.205198	7325.619289	8.775616	-0.048155	4.614190
231.135645	7333.695451	8.780621	-0.048147	4.616654
231.255477	7341.592692	8.785626	-0.048175	4.619063
231.581818	7349.687829	8.790631	-0.048241	4.621530
231.565700	7357.617044	8.795635	-0.048244	4.623946
231.795896	7365.689071	8.800640	-0.048292	4.626404
231.928773	7373.691506	8.805645	-0.048323	4.628840
231.997629	7381.721747	8.810650	-0.048341	4.631282
232.193947	7389.809863	8.815655	-0.048383	4.633741
232.439294	7397.782199	8.820659	-0.048434	4.636163
232.664947	7405.700160	8.825664	-0.048482	4.638568
232.744901	7413.808238	8.830669	-0.048502	4.641029
232.903361	7421.746877	8.835674	-0.048537	4.643437
232.933948	7429.820189	8.840679	-0.048548	4.645885
233.015669	7437.805176	8.845683	-0.048569	4.648305
233.126367	7445.841870	8.850688	-0.048595	4.650739
233.221411	7453.890000	8.855693	-0.048618	4.653176
233.442594	7461.902550	8.860698	-0.048665	4.655600
233.777766	7469.907368	8.865703	-0.048733	4.658021
233.670007	7477.873562	8.870707	-0.048718	4.660429
233.970778	7485.916722	8.875712	-0.048780	4.662858
234.036599	7493.908448	8.880717	-0.048798	4.665271
234.096016	7501.933292	8.885722	-0.048814	4.667693
234.281739	7509.972207	8.890727	-0.048854	4.670117
234.469309	7518.037142	8.895731	-0.048895	4.672549
234.604486	7526.093671	8.900736	-0.048925	4.674976
234.705247	7534.065100	8.905741	-0.048950	4.677376
234.783339	7542.023955	8.910746	-0.048970	4.679772
235.095429	7550.044233	8.915751	-0.049033	4.682184
234.905906	7557.995368	8.920755	-0.049004	4.684575
235.039562	7566.052110	8.925760	-0.049034	4.686997
235.120034	7574.079495	8.930765	-0.049054	4.689408
235.247850	7582.075976	8.935770	-0.049084	4.691808
235.493902	7590.094010	8.940775	-0.049135	4.694214
235.608208	7598.147678	8.945779	-0.049162	4.696629
235.586145	7606.121285	8.950784	-0.049163	4.699019
235.640503	7614.131793	8.955789	-0.049179	4.701419
235.945434	7622.124219	8.960794	-0.049241	4.703812
236.137077	7630.193050	8.965799	-0.049282	4.706226
236.100020	7638.146429	8.970803	-0.049281	4.708605
236.221222	7646.206354	8.975808	-0.049309	4.711015
236.498729	7654.264379	8.980813	-0.049366	4.713422
236.372193	7662.258550	8.985818	-0.049348	4.715810
236.567921	7670.305427	8.990823	-0.049390	4.718212
236.716772	7678.265038	8.995827	-0.049423	4.720587
237.038037	7686.276291	9.000832	-0.049489	4.722975
237.022353	7694.283505	9.005837	-0.049491	4.725362
237.156263	7702.320234	9.010842	-0.049522	4.727756
237.516417	7710.343264	9.015847	-0.049594	4.730144
237.402517	7718.417430	9.020851	-0.049579	4.732547
237.609589	7726.389581	9.025856	-0.049623	4.734918
237.810603	7734.438230	9.030861	-0.049666	4.737310
237.938046	7742.391513	9.035866	-0.049695	4.739673
238.259845	7750.489595	9.040871	-0.049760	4.742078
238.366774	7758.398227	9.045875	-0.049786	4.744425
238.367591	7766.466514	9.050880	-0.049791	4.746819
238.526929	7774.483736	9.055885	-0.049826	4.749196
238.762945	7782.524852	9.060890	-0.049876	4.751579
239.007664	7790.601824	9.065895	-0.049927	4.753971
238.767335	7798.562485	9.070899	-0.049888	4.756329
238.936835	7806.498001	9.075904	-0.049925	4.758677
239.066915	7814.528886	9.080909	-0.049955	4.761052
239.186247	7822.494003	9.085914	-0.049982	4.763407
239.335992	7830.564928	9.090919	-0.050016	4.765791
239.484478	7838.576513	9.095923	-0.050049	4.768157
239.950654	7846.600365	9.100928	-0.050141	4.770524
239.790286	7854.672250	9.105933	-0.050117	4.772907
239.996806	7862.644869	9.110938	-0.050161	4.775257
240.192648	7870.666915	9.115943	-0.050203	4.777621
240.342529	7878.676506	9.120947	-0.050236	4.779981
240.624641	7886.631467	9.125952	-0.050294	4.782322
240.558739	7894.689635	9.130957	-0.050287	4.784694
240.790169	7902.656149	9.135962	-0.050336	4.787037
241.080553	7910.717764	9.140967	-0.050396	4.789406
241.000186	7918.769682	9.145971	-0.050386	4.791773
241.076339	7926.788497	9.150976	-0.050406	4.794128
241.305865	7934.812486	9.155981	-0.050454	4.796483
241.336953	7942.757749	9.160986	-0.050465	4.798815
241.596959	7950.800845	9.165991	-0.050519	4.801173
241.577271	7958.709517	9.170995	-0.050521	4.803492
241.479673	7966.804101	9.176000	-0.050508	4.805864
241.965694	7974.824378	9.181005	-0.050604	4.808211
242.098297	7982.837823	9.186010	-0.050635	4.810556
242.150805	7990.254163	9.191015	-0.050649	4.812726
242.268003	7994.779573	9.196019	-0.050675	4.814049

242.396417	7997.230742	9.201024	-0.050700	4.814765
242.490876	7998.499684	9.206029	-0.050719	4.815136
242.594571	7998.918895	9.211034	-0.050739	4.815258
242.758095	7999.961647	9.216039	-0.050770	4.815562
242.637452	7999.894566	9.221043	-0.050748	4.815543
242.624071	7999.915730	9.226048	-0.050746	4.815549
242.838808	7999.941679	9.231053	-0.050786	4.815556
243.054885	7999.921731	9.236058	-0.050827	4.815549
242.785441	7999.965420	9.241063	-0.050777	4.815563
242.737881	7999.909140	9.246067	-0.050768	4.815547
243.033143	7999.862719	9.251072	-0.050823	4.815532
243.078795	7999.919016	9.256077	-0.050832	4.815548
242.974645	7999.960059	9.261082	-0.050813	4.815560
243.067545	7999.953054	9.266087	-0.050831	4.815558
242.890759	7999.960877	9.271091	-0.050798	4.815561
243.037882	7999.948349	9.276096	-0.050826	4.815557
243.165500	7999.932300	9.281101	-0.050850	4.815551
243.285296	7999.927869	9.286106	-0.050872	4.815549
243.357039	7999.962168	9.291111	-0.050886	4.815559
243.195208	7999.941401	9.296115	-0.050856	4.815554
243.515642	7999.978685	9.301120	-0.050916	4.815563
243.412866	7999.926844	9.306125	-0.050897	4.815548
243.416498	7999.937607	9.311130	-0.050898	4.815552
243.604118	7999.979133	9.316135	-0.050934	4.815563
243.561924	7999.916533	9.321139	-0.050926	4.815545
243.456322	7999.968231	9.326144	-0.050907	4.815560
243.758317	7999.944345	9.331149	-0.050963	4.815552
243.750452	7999.894051	9.336154	-0.050962	4.815537
243.667938	7999.929039	9.341159	-0.050947	4.815548
243.768910	7999.921098	9.346163	-0.050966	4.815545
243.880675	7999.950710	9.351168	-0.050987	4.815553
243.890212	7999.950890	9.356173	-0.050989	4.815553
243.650677	7999.929924	9.361178	-0.050945	4.815548
243.747386	7999.957155	9.366183	-0.050963	4.815556
243.776111	7999.924543	9.371187	-0.050969	4.815546
243.849228	7999.985562	9.376192	-0.050983	4.815563
243.834215	7999.971459	9.381197	-0.050980	4.815559
244.097488	7999.955486	9.386202	-0.051029	4.815553
244.174205	7999.990934	9.391207	-0.051044	4.815563
243.901041	7999.944857	9.396211	-0.050993	4.815551
243.955555	7999.984215	9.401216	-0.051004	4.815562
244.111690	8000.001736	9.406221	-0.051033	4.815567
243.889317	7999.950080	9.411226	-0.050992	4.815553
243.917380	7999.971920	9.416231	-0.050997	4.815559
244.086074	7999.971491	9.421235	-0.051029	4.815558
244.007204	7999.960619	9.426240	-0.051015	4.815555
243.936164	7999.958418	9.431245	-0.051002	4.815555
244.010303	7999.952176	9.436250	-0.051016	4.815553
244.045745	7999.983748	9.441255	-0.051023	4.815562
243.996613	7999.957342	9.446259	-0.051014	4.815554
244.133470	7999.988431	9.451264	-0.051040	4.815563
244.212613	7999.967320	9.456269	-0.051055	4.815556
244.106843	7999.947466	9.461274	-0.051035	4.815551
244.280874	7999.964211	9.466279	-0.051068	4.815555
244.294311	7999.943097	9.471283	-0.051071	4.815549
244.156098	7999.970770	9.476288	-0.051045	4.815557
244.310601	7999.975449	9.481293	-0.051074	4.815558
244.310812	7999.968002	9.486298	-0.051075	4.815556
244.393708	7999.997144	9.491303	-0.051090	4.815564
244.088180	7999.946267	9.496307	-0.051034	4.815551
244.163041	7999.973142	9.501312	-0.051048	4.815558
244.393743	7999.951299	9.506317	-0.051091	4.815551
244.174489	7999.952020	9.511322	-0.051051	4.815552
244.193188	7999.999338	9.516327	-0.051055	4.815566
244.295091	7999.964715	9.521331	-0.051074	4.815555
244.456637	7999.970578	9.526336	-0.051104	4.815556
244.491275	7999.977575	9.531341	-0.051111	4.815558
244.514827	7999.925656	9.536346	-0.051115	4.815542
244.674742	7999.971005	9.541351	-0.051146	4.815555
244.525362	7999.925878	9.546355	-0.051118	4.815542
244.496686	7999.983102	9.551360	-0.051113	4.815559
244.707261	7999.970542	9.556365	-0.051152	4.815555
244.445819	7999.981254	9.561370	-0.051104	4.815559
244.649853	8000.033730	9.566375	-0.051142	4.815573
244.627624	7999.962910	9.571379	-0.051138	4.815553
244.553792	8000.017262	9.576384	-0.051125	4.815569
244.347932	7999.963738	9.581389	-0.051087	4.815554
244.504991	7999.956713	9.586394	-0.051116	4.815552
244.607958	8000.029967	9.591399	-0.051136	4.815572
244.295079	8000.005667	9.596403	-0.051078	4.815567
244.274883	8000.012838	9.601408	-0.051075	4.815569
244.585841	7999.988032	9.606413	-0.051133	4.815560
244.673898	7999.972406	9.611418	-0.051149	4.815555
244.491124	7999.991876	9.616423	-0.051116	4.815562
244.353401	7999.939464	9.621427	-0.051090	4.815547
244.493261	7999.943905	9.626432	-0.051117	4.815548
244.698054	7999.973967	9.631437	-0.051155	4.815556
244.623436	7999.946077	9.636442	-0.051141	4.815548
244.581063	7999.987059	9.641447	-0.051134	4.815560
244.699635	7999.980474	9.646451	-0.051156	4.815557
244.545790	7999.990805	9.651456	-0.051128	4.815561
244.612320	7999.965217	9.656461	-0.051140	4.815553
244.538593	7999.952292	9.661466	-0.051127	4.815550
244.803153	7999.987601	9.666471	-0.051177	4.815559
244.807529	7999.957796	9.671475	-0.051178	4.815550
244.724352	7999.979958	9.676480	-0.051162	4.815557
244.538095	7999.991896	9.681485	-0.051128	4.815562
244.517131	7999.978764	9.686490	-0.051124	4.815558
244.681769	7999.984677	9.691495	-0.051155	4.815559
244.607491	7999.964268	9.696499	-0.051142	4.815553
244.781934	7999.945780	9.701504	-0.051175	4.815547
244.822986	7999.976376	9.706509	-0.051182	4.815556
244.962733	7999.975476	9.711514	-0.051209	4.815555
245.054094	8000.018640	9.716519	-0.051226	4.815567
244.870160	7999.980423	9.721523	-0.051192	4.815557
244.952993	8000.012769	9.726528	-0.051208	4.815566
244.914433	8000.019640	9.731533	-0.051201	4.815568
244.836716	7999.963933	9.736538	-0.051187	4.815552
245.132031	7999.992269	9.741543	-0.051242	4.815559
245.015861	7999.979720	9.746547	-0.051221	4.815556
244.980504	8000.014409	9.751552	-0.051214	4.815566
244.902821	8000.001420	9.756557	-0.051200	4.815562
244.824887	7999.955321	9.761562	-0.051186	4.815549
244.907907	8000.009028	9.766567	-0.051202	4.815565
244.990769	7999.987978	9.771571	-0.051217	4.815558
244.937935	8000.023450	9.776576	-0.051208	4.815569
244.918993	7999.994332	9.781581	-0.051205	4.815560
244.911240	7999.979279	9.786586	-0.051203	4.815556
245.328453	8000.016012	9.791591	-0.051281	4.815565
245.158924	8000.008999	9.796595	-0.051250	4.815563
245.107909	8000.041298	9.801600	-0.051241	4.815573
245.382521	7999.989202	9.806605	-0.051292	4.815557
245.209930	7999.973596	9.811610	-0.051260	4.815553
245.417718	8000.016524	9.816615	-0.051299	4.815564
245.137522	7999.981008	9.821619	-0.051248	4.815555
245.079486	8000.013191	9.826624	-0.051237	4.815565
245.120958	8000.013893	9.831629	-0.051245	4.815565
245.077087	7999.973689	9.836634	-0.051237	4.815553
245.290791	8000.002830	9.841639	-0.051277	4.815561
245.127254	8000.013002	9.846643	-0.051247	4.815565
245.208731	7999.998337	9.851648	-0.051263	4.815560
245.384727	8000.015116	9.856653	-0.051296	4.815564
245.156221	7999.994326	9.861658	-0.051253	4.815559
245.169104	8000.011648	9.866663	-0.051256	4.815564
245.149424	7999.998536	9.871667	-0.051253	4.815560
245.246867	7999.988403	9.876672	-0.051271	4.815557
245.272830	7999.981376	9.881677	-0.051276	4.815555
245.357402	7999.958218	9.886682	-0.051292	4.815547
245.437694	8000.027901	9.891687	-0.051307	4.815567
245.393965	7999.991970	9.896691	-0.051300	4.815557
245.227108	7999.977526	9.901696	-0.051269	4.815554
245.256858	8000.011142	9.906701	-0.051275	4.815563
245.371838	8000.005567	9.911706	-0.051296	4.815561
245.299645	8000.003346	9.916711	-0.051283	4.815561
245.239188	7999.971414	9.921715	-0.051272	4.815552
245.371566	8000.024859	9.926720	-0.051297	4.815567
245.311218	8000.021764	9.931725	-0.051286	4.815566
245.178375	7999.967292	9.936730	-0.051262	4.815551
245.426068	8000.023687	9.941735	-0.051308	4.815566
245.566589	8000.003578	9.946739	-0.051335	4.815560
245.290739	8000.021529	9.951744	-0.051283	4.815566
245.422368	8000.019429	9.956749	-0.051308	4.815565
245.262999	8000.006174	9.961754	-0.051279	4.815562
245.321750	8000.047739	9.966759	-0.051290	4.815574
245.396573	7999.995588	9.971763	-0.051304	4.815558
245.513057	8000.024212	9.976768	-0.051326	4.815566
245.613834	8000.019473	9.981773	-0.051345	4.815564
245.329349	7999.989226	9.986778	-0.051293	4.815557
245.441679	8000.014578	9.991783	-0.051314	4.815563
245.509984	8000.013581	9.996787	-0.051327	4.815563
245.324733	8000.007380	10.001792	-0.051293	4.815562
245.287438	8000.019611	10.006797	-0.051286	4.815566
245.385430	8000.016963	10.011802	-0.051304	4.815564
245.390335	8000.045902	10.016807	-0.051306	4.815573
245.359993	7999.995239	10.021811	-0.051300	4.815558
245.442384	8000.026510	10.026816	-0.051316	4.815567
245.715375	8000.055552	10.031821	-0.051367	4.815574
245.513680	8000.024519	10.036826	-0.051330	4.815566
245.533374	8000.064379	10.041831	-0.051334	4.815577
245.478239	8000.001563	10.046835	-0.051324	4.815559
245.473192	8000.006846	10.051840	-0.051323	4.815561
245.499866	8000.021189	10.056845	-0.051328	4.815565
245.345209	7999.949274	10.061850	-0.051300	4.815545
245.573456	8000.014963	10.066855	-0.051343	4.815563
245.404911	7999.988744	10.071859	-0.051311	4.815556
245.391706	8000.012048	10.076864	-0.051309	4.815563
245.565007	7999.997813	10.081869	-0.051342	4.815558
245.234315	7999.995646	10.086874	-0.051281	4.815559
245.357749	8000.007296	10.091879	-0.051304	4.815562
245.431569	8000.002118	10.096883	-0.051318	4.815560
245.456151	8000.000408	10.101888	-0.051323	4.815559
245.539795	8000.025292	10.106893	-0.051339	4.815566
245.517878	7999.985445	10.111898	-0.051335	4.815554
245.568140	7999.996969	10.116903	-0.051344	4.815557
245.521945	7999.962066	10.121907	-0.051336	4.815547
245.716032	8000.019723	10.126912	-0.051373	4.815563
245.519812	8000.011206	10.131917	-0.051336	4.815562
245.644514	7999.982295	10.136922	-0.051360	4.815553
245.725457	8000.030631	10.141927	-0.051375	4.815567
245.519866	8000.027301	10.146931	-0.051337	4.815567
245.648004	8000.042232	10.151936	-0.051361	4.815570
245.715631	8000.040156	10.156941	-0.051374	4.815569
245.621091	7999.977765	10.161946	-0.051357	4.815552
245.659786	8000.023275	10.166951	-0.051364	4.815565
245.436467	8000.017520	10.171955	-0.051323	4.815564
245.373327	7999.996224	10.176960	-0.051312	4.815558
245.634964	8000.035760	10.181965	-0.051361	4.815568
245.393532	8000.017962	10.186970	-0.051316	4.815564
245.606873	8000.031079	10.191975	-0.051356	4.815567
245.850415	8000.015855	10.196979	-0.051402	4.815562
245.863583	8000.041725	10.201984	-0.051404	4.815569
245.760822	8000.037937	10.206989	-0.051385	4.815568
245.845529	8000.036141	10.211994	-0.051401	4.815567
245.918171	8000.045894	10.216999	-0.051415	4.815570
245.812162	8000.042053	10.222003	-0.051396	4.815569
245.545158	8000.032381	10.227008	-0.051346	4.815568
245.870202	8000.047322	10.232013	-0.051407	4.815571
245.633957	7999.999705	10.237018	-0.051363	4.815558
245.681499	8000.047496	10.242023	-0.051373	4.815572
245.640787	8000.018022	10.247027	-0.051365	4.815563
245.788954	8000.036483	10.252032	-0.051393	4.815568
245.822907	8000.044538	10.257037	-0.051400	4.815570
245.826920	7999.998706	10.262042	-0.051401	4.815557
245.882856	8000.035954	10.267047	-0.051412	4.815567
245.812006	8000.039095	10.272051	-0.051399	4.815568
245.676226	8000.045447	10.277056	-0.051374	4.815571
245.811407	8000.031659	10.282061	-0.051399	4.815566
245.759109	8000.019083	10.287066	-0.051390	4.815563
245.831612	8000.016019	10.292071	-0.051403	4.815562
246.091411	7999.996788	10.297075	-0.051452	4.815555
245.869062	8000.028427	10.302080	-0.051411	4.815565
245.940267	8000.044565	10.307085	-0.051424	4.815569
245.853325	7999.997249	10.312090	-0.051409	4.815556
246.119378	8000.032586	10.317095	-0.051458	4.815565
245.974941	8000.027050	10.322099	-0.051432	4.815564
245.922246	8000.037962	10.327104	-0.051422	4.815567
246.011358	8000.042645	10.332109	-0.051439	4.815568
245.857352	8000.024137	10.337114	-0.051411	4.815564
245.708002	8000.037744	10.342119	-0.051383	4.815568
245.666748	8000.013601	10.347123	-0.051376	4.815562
245.750302	8000.026736	10.352128	-0.051392	4.815565
245.821600	8000.001226	10.357133	-0.051405	4.815557
245.825595	7999.998112	10.362138	-0.051406	4.815556
245.991360	8000.048900	10.367143	-0.051437	4.815570
245.898445	8000.023913	10.372147	-0.051420	4.815563
245.797555	8000.024428	10.377152	-0.051402	4.815564
246.057541	8000.034035	10.382157	-0.051451	4.815566
246.011957	8000.004481	10.387162	-0.051442	4.815557
245.993205	8000.040510	10.392167	-0.051439	4.815568
245.922378	8000.014816	10.397171	-0.051426	4.815561
246.036789	8000.022048	10.402176	-0.051448	4.815562
245.897390	8000.036885	10.407181	-0.051422	4.815567
245.895696	8000.019795	10.412186	-0.051422	4.815562
245.938440	8000.023721	10.417191	-0.051430	4.815563
245.872729	8000.018402	10.422195	-0.051418	4.815562
245.806329	8000.015207	10.427200	-0.051406	4.815561
246.081779	8000.030407	10.432205	-0.051458	4.815564
246.085153	8000.025147	10.437210	-0.051459	4.815563
246.071236	8000.034556	10.442215	-0.051457	4.815566
245.906535	8000.003058	10.447219	-0.051426	4.815557
246.109405	8000.021345	10.452224	-0.051464	4.815562
246.276471	8000.059339	10.457229	-0.051496	4.815572
246.196655	8000.019615	10.462234	-0.051481	4.815561
246.028289	8000.016891	10.467239	-0.051450	4.815561
246.017165	8000.022074	10.472243	-0.051448	4.815562
245.892036	8000.009378	10.477248	-0.051425	4.815559
246.197773	8000.046431	10.482253	-0.051482	4.815568
245.964211	8000.003129	10.487258	-0.051439	4.815557
245.816055	8000.049862	10.492263	-0.051412	4.815571
245.840435	8000.038537	10.497267	-0.051417	4.815568
246.041531	8000.039708	10.502272	-0.051454	4.815567
246.034665	8000.055640	10.507277	-0.051453	4.815572
245.923154	8000.014331	10.512282	-0.051433	4.815560
246.081452	8000.042570	10.517287	-0.051463	4.815568
246.278783	8000.026592	10.522291	-0.051500	4.815562
246.013699	8000.029766	10.527296	-0.051451	4.815564
246.207090	8000.039355	10.532301	-0.051487	4.815566
246.080797	7999.999940	10.537306	-0.051464	4.815555
246.264520	8000.031798	10.542311	-0.051498	4.815564
245.926010	8000.002803	10.547315	-0.051435	4.815557
246.039152	8000.005742	10.552320	-0.051457	4.815557
246.156374	8000.003408	10.557325	-0.051479	4.815556
246.149800	7999.995850	10.562330	-0.051478	4.815554
246.234926	8000.031439	10.567335	-0.051494	4.815564
246.311486	8000.007082	10.572339	-0.051509	4.815556
246.302574	8000.016573	10.577344	-0.051507	4.815559
246.117843	8000.033874	10.582349	-0.051473	4.815565
246.099016	7999.986601	10.587354	-0.051470	4.815551
246.280502	8000.044055	10.592359	-0.051504	4.815567
246.116254	8000.032855	10.597363	-0.051474	4.815565
246.314045	8000.035040	10.602368	-0.051511	4.815564
246.219525	8000.049541	10.607373	-0.051493	4.815569
246.179165	8000.031820	10.612378	-0.051486	4.815564
246.430237	8000.020991	10.617383	-0.051533	4.815560
246.409738	8000.032429	10.622387	-0.051530	4.815563
246.179593	8000.030833	10.627392	-0.051487	4.815564
246.319257	8000.038478	10.632397	-0.051513	4.815565
246.397958	8000.001340	10.637402	-0.051528	4.815554
246.551200	8000.044449	10.642407	-0.051557	4.815566
246.359074	8000.033862	10.647411	-0.051522	4.815564
246.222804	8000.038070	10.652416	-0.051497	4.815566
246.403376	8000.042110	10.657421	-0.051531	4.815566
246.200453	8000.009988	10.662426	-0.051493	4.815557
246.241880	8000.053407	10.667431	-0.051501	4.815570
246.401548	8000.019728	10.672435	-0.051531	4.815559
246.479863	8000.040254	10.677440	-0.051546	4.815565
246.555064	8000.052186	10.682445	-0.051560	4.815568
246.513417	8000.013084	10.687450	-0.051553	4.815557
246.639949	8000.060030	10.692455	-0.051577	4.815570
246.398528	8000.024074	10.697459	-0.051532	4.815561
246.402808	8000.051936	10.702464	-0.051533	4.815569
246.521661	8000.054969	10.707469	-0.051555	4.815569
246.401991	8000.024205	10.712474	-0.051533	4.815561
246.621575	8000.042766	10.717479	-0.051575	4.815565
246.564632	8000.009822	10.722483	-0.051564	4.815556
246.325356	8000.004873	10.727488	-0.051520	4.815555
246.323112	8000.017677	10.732493	-0.051520	4.815559
246.291999	8000.030009	10.737498	-0.051514	4.815563
246.481217	8000.071570	10.742503	-0.051550	4.815574
246.394335	8000.037069	10.747507	-0.051534	4.815564
246.280766	8000.029900	10.752512	-0.051513	4.815563
246.524002	8000.049915	10.757517	-0.051559	4.815567
246.423243	8000.005576	10.762522	-0.051540	4.815555
246.482090	8000.056756	10.767527	-0.051551	4.815570
246.484027	8000.072832	10.772531	-0.051552	4.815574
246.375570	8000.049727	10.777536	-0.051532	4.815568
246.518150	8000.077711	10.782541	-0.051559	4.815576
246.314463	8000.054119	10.787546	-0.051521	4.815570
246.396847	8000.080052	10.792551	-0.051537	4.815577
246.362100	8000.045334	10.797555	-0.051531	4.815567
246.432721	8000.033696	10.802560	-0.051544	4.815563
246.712737	8000.046836	10.807565	-0.051597	4.815566
246.559008	8000.016584	10.812570	-0.051568	4.815557
246.522038	8000.077948	10.817575	-0.051562	4.815576
246.556964	8000.055047	10.822579	-0.051568	4.815569
246.432546	8000.048769	10.827584	-0.051546	4.815567
246.465982	8000.054679	10.832589	-0.051552	4.815569
246.338267	8000.024852	10.837594	-0.051529	4.815561
246.548723	8000.076371	10.842599	-0.051568	4.815575
246.552179	8000.070045	10.847603	-0.051569	4.815573
246.446951	8000.052332	10.852608	-0.051550	4.815568
246.627446	8000.086275	10.857613	-0.051584	4.815577
246.723511	8000.057965	10.862618	-0.051602	4.815569
246.527265	8000.079349	10.867623	-0.051565	4.815576
246.514610	8000.065283	10.872627	-0.051563	4.815572
246.761677	8000.068274	10.877632	-0.051610	4.815572
246.733794	8000.078523	10.882637	-0.051605	4.815575
246.701398	8000.038504	10.887642	-0.051599	4.815563
246.748176	8000.087351	10.892647	-0.051608	4.815577
246.638200	8000.026842	10.897651	-0.051588	4.815560
246.434105	8000.029943	10.902656	-0.051550	4.815562
246.479402	8000.045658	10.907661	-0.051559	4.815566
246.369616	8000.042823	10.912666	-0.051539	4.815566
246.562861	8000.071634	10.917671	-0.051575	4.815573
246.656770	8000.060376	10.922675	-0.051593	4.815570
246.744416	8000.072512	10.927680	-0.051609	4.815573
246.582525	8000.068825	10.932685	-0.051579	4.815572
246.435199	8000.072853	10.937690	-0.051552	4.815574
246.573935	8000.083686	10.942695	-0.051578	4.815577
246.470284	8000.064931	10.947699	-0.051559	4.815572
246.523390	8000.064755	10.952704	-0.051570	4.815572
246.718221	8000.066893	10.957709	-0.051606	4.815571
246.819347	8000.060025	10.962714	-0.051625	4.815569
246.757876	8000.070794	10.967719	-0.051614	4.815572
246.705117	8000.062481	10.972723	-0.051605	4.815570
246.622400	8000.065428	10.977728	-0.051589	4.815571
246.676476	8000.065267	10.982733	-0.051600	4.815571
246.487557	8000.029100	10.987738	-0.051565	4.815561
246.801629	8000.050273	10.992743	-0.051624	4.815566
246.626849	8000.053851	10.997747	-0.051591	4.815568
246.544035	8000.054660	11.002752	-0.051576	4.815568
246.887803	8000.064570	11.007757	-0.051640	4.815570
246.719355	8000.025533	11.012762	-0.051609	4.815559
246.795039	8000.064173	11.017767	-0.051624	4.815570
246.695897	8000.081802	11.022771	-0.051606	4.815576
246.727863	8000.073805	11.027776	-0.051612	4.815573
246.877419	8000.084816	11.032781	-0.051640	4.815576
246.797958	8000.055776	11.037786	-0.051625	4.815567
246.840567	8000.083196	11.042791	-0.051634	4.815575
246.861814	8000.046188	11.047795	-0.051638	4.815564
246.532656	8000.047246	11.052800	-0.051577	4.815566
246.597955	8000.066493	11.057805	-0.051589	4.815572
246.467658	8000.025943	11.062810	-0.051565	4.815560
246.531131	8000.050500	11.067815	-0.051577	4.815567
246.512113	8000.042738	11.072819	-0.051574	4.815565
246.533544	8000.050589	11.077824	-0.051578	4.815567
246.746571	8000.048752	11.082829	-0.051618	4.815566
246.500259	8000.040483	11.087834	-0.051573	4.815564
246.672669	8000.063614	11.092839	-0.051605	4.815570
246.680010	8000.032787	11.097843	-0.051607	4.815561
246.643448	8000.045031	11.102848	-0.051600	4.815565
246.692494	8000.059740	11.107853	-0.051610	4.815569
246.704883	8000.053560	11.112858	-0.051612	4.815567
246.806678	8000.072334	11.117863	-0.051632	4.815572
246.739919	8000.037093	11.122867	-0.051619	4.815562
246.619060	8000.054369	11.127872	-0.051597	4.815568
246.720421	8000.077408	11.132877	-0.051616	4.815574
246.701071	8000.037601	11.137882	-0.051613	4.815562
246.696346	8000.063181	11.142887	-0.051612	4.815570
246.920121	8000.022004	11.147891	-0.051654	4.815557
246.770849	8000.035611	11.152896	-0.051627	4.815562
246.757322	8000.061047	11.157901	-0.051625	4.815569
246.661533	8000.041352	11.162906	-0.051607	4.815564
246.658058	8000.076563	11.167911	-0.051607	4.815574
246.719768	8000.073324	11.172915	-0.051619	4.815573
246.659746	8000.044601	11.177920	-0.051608	4.815565
246.749546	8000.054636	11.182925	-0.051625	4.815567
246.745525	8000.036439	11.187930	-0.051624	4.815562
246.824087	8000.068718	11.192935	-0.051639	4.815571
246.941814	8000.041830	11.197939	-0.051661	4.815562
246.928653	8000.037368	11.202944	-0.051659	4.815561
246.930111	8000.070524	11.207949	-0.051660	4.815571
246.877269	8000.010947	11.212954	-0.051650	4.815554
246.683344	8000.065476	11.217959	-0.051614	4.815571
246.691721	8000.037870	11.222963	-0.051616	4.815562
246.732503	8000.018269	11.227968	-0.051624	4.815557
247.002741	8000.078242	11.232973	-0.051675	4.815573
246.890227	8000.031574	11.237978	-0.051654	4.815560
246.859271	8000.073813	11.242983	-0.051648	4.815572
246.820382	8000.040095	11.247987	-0.051641	4.815562
246.692438	8000.060458	11.252992	-0.051618	4.815569
246.689068	8000.080720	11.257997	-0.051618	4.815575
246.749723	8000.057171	11.263002	-0.051629	4.815568
246.903320	8000.058636	11.268007	-0.051658	4.815567
246.759505	8000.047769	11.273011	-0.051632	4.815565
246.716001	8000.044947	11.278016	-0.051624	4.815564
246.963099	8000.046871	11.283021	-0.051670	4.815564
246.959553	8000.057517	11.288026	-0.051670	4.815567
247.018614	8000.055303	11.293031	-0.051681	4.815566
246.849324	8000.047223	11.298035	-0.051650	4.815564
246.635627	8000.024535	11.303040	-0.051610	4.815559
246.897829	8000.067288	11.308045	-0.051659	4.815570
246.870732	8000.025219	11.313050	-0.051655	4.815558
247.025658	8000.058746	11.318055	-0.051684	4.815567
246.840807	8000.065364	11.323059	-0.051650	4.815570
246.700566	8000.051351	11.328064	-0.051624	4.815566
247.059000	8000.084996	11.333069	-0.051691	4.815574
246.894052	8000.026792	11.338074	-0.051660	4.815558
246.708303	8000.072911	11.343079	-0.051626	4.815572
246.936292	8000.032871	11.348083	-0.051669	4.815560
247.018989	8000.051334	11.353088	-0.051684	4.815565
246.906820	8000.063411	11.358093	-0.051664	4.815569
246.872975	8000.025504	11.363098	-0.051658	4.815558
246.880189	8000.060890	11.368103	-0.051659	4.815568
247.068370	8000.046900	11.373107	-0.051695	4.815563
246.883032	8000.005451	11.378112	-0.051660	4.815552
246.927864	8000.048927	11.383117	-0.051669	4.815564
246.914311	8000.029507	11.388122	-0.051667	4.815559
246.837122	8000.054971	11.393127	-0.051653	4.815567
246.882220	8000.045052	11.398131	-0.051661	4.815563
246.631993	8000.047399	11.403136	-0.051615	4.815565
246.672704	8000.040612	11.408141	-0.051623	4.815563
246.741009	8000.047092	11.413146	-0.051636	4.815565
246.843298	8000.081895	11.418151	-0.051655	4.815574
246.751244	8000.087893	11.423155	-0.051639	4.815577
246.719521	8000.042544	11.428160	-0.051633	4.815563
246.905981	8000.041341	11.433165	-0.051668	4.815562
246.767832	8000.043382	11.438170	-0.051642	4.815563
246.594448	8000.059800	11.443175	-0.051610	4.815569
246.766866	8000.043416	11.448179	-0.051643	4.815563
246.821114	8000.061414	11.453184	-0.051653	4.815568
246.773497	8000.088429	11.458189	-0.051645	4.815577
246.762140	8000.055161	11.463194	-0.051643	4.815567
246.980171	8000.098262	11.468199	-0.051684	4.815578
246.782903	8000.059822	11.473203	-0.051647	4.815568
246.684636	8000.051834	11.478208	-0.051629	4.815566
247.008611	8000.080645	11.483213	-0.051690	4.815573
246.894181	8000.064917	11.488218	-0.051669	4.815569
246.816404	8000.071148	11.493223	-0.051655	4.815571
247.029225	8000.060764	11.498227	-0.051695	4.815567
246.659399	8000.049410	11.503232	-0.051626	4.815566
246.718208	8000.051463	11.508237	-0.051637	4.815566
246.750178	8000.072301	11.513242	-0.051643	4.815572
246.933718	8000.089207	11.518247	-0.051678	4.815576
246.857409	8000.073034	11.523251	-0.051664	4.815572
246.767012	8000.061971	11.528256	-0.051647	4.815569
246.972027	8000.058935	11.533261	-0.051686	4.815567
247.119135	8000.020779	11.538266	-0.051714	4.815555
246.986536	8000.053882	11.543271	-0.051689	4.815565
246.992387	8000.051866	11.548275	-0.051690	4.815565
247.131003	8000.059495	11.553280	-0.051717	4.815566
247.042430	8000.081569	11.558285	-0.051700	4.815573
246.943183	8000.046865	11.563290	-0.051682	4.815563
246.904874	8000.086848	11.568295	-0.051675	4.815575
247.100233	8000.065499	11.573299	-0.051712	4.815568
246.895289	8000.056837	11.578304	-0.051674	4.815567
247.033397	8000.067661	11.583309	-0.051700	4.815569
246.968778	8000.064495	11.588314	-0.051688	4.815568
247.015047	8000.064207	11.593319	-0.051697	4.815568
247.183566	8000.069120	11.598323	-0.051729	4.815569
247.040926	8000.066816	11.603328	-0.051703	4.815569
247.180190	8000.099019	11.608333	-0.051729	4.815577
246.949719	8000.040812	11.613338	-0.051686	4.815562
247.024292	8000.060210	11.618343	-0.051700	4.815567
246.864092	8000.044803	11.623347	-0.051671	4.815563
246.740430	8000.062032	11.628352	-0.051648	4.815569
246.858460	8000.083208	11.633357	-0.051670	4.815574
246.812621	8000.058989	11.638362	-0.051662	4.815567
246.802166	8000.067387	11.643367	-0.051660	4.815570
246.725834	8000.072573	11.648371	-0.051647	4.815572
246.799808	8000.075942	11.653376	-0.051661	4.815572
246.888748	8000.092371	11.658381	-0.051677	4.815577
246.612156	8000.075063	11.663386	-0.051626	4.815573
246.821740	8000.076374	11.668391	-0.051666	4.815572
246.904423	8000.076681	11.673395	-0.051681	4.815572
246.702727	8000.068073	11.678400	-0.051644	4.815571
247.057011	8000.089903	11.683405	-0.051710	4.815575
246.979380	8000.047008	11.688410	-0.051696	4.815563
247.091460	8000.084107	11.693415	-0.051717	4.815573
247.136105	8000.068841	11.698419	-0.051726	4.815569
246.942093	8000.065697	11.703424	-0.051690	4.815569
247.058375	8000.084709	11.708429	-0.051712	4.815574
246.806041	8000.030417	11.713434	-0.051665	4.815559
247.128930	8000.077367	11.718439	-0.051726	4.815571
247.204165	8000.087164	11.723443	-0.051740	4.815574
247.063175	8000.025079	11.728448	-0.051714	4.815556
246.808697	8000.081823	11.733453	-0.051667	4.815574
246.886518	8000.071371	11.738458	-0.051682	4.815571
247.048271	8000.085785	11.743463	-0.051712	4.815574
247.090034	8000.070472	11.748467	-0.051720	4.815569
246.974882	8000.059005	11.753472	-0.051699	4.815567
247.271667	8000.086305	11.758477	-0.051754	4.815573
247.079392	8000.066101	11.763482	-0.051719	4.815568
247.108577	8000.066602	11.768487	-0.051725	4.815568
247.053580	8000.061457	11.773491	-0.051715	4.815567
246.999365	8000.064868	11.778496	-0.051705	4.815568
247.016174	8000.075848	11.783501	-0.051708	4.815571
247.091660	8000.058949	11.788506	-0.051723	4.815566
247.216340	8000.073826	11.793511	-0.051746	4.815570
247.062716	8000.080954	11.798515	-0.051718	4.815572
247.131567	8000.043655	11.803520	-0.051731	4.815561
247.351438	8000.062223	11.808525	-0.051772	4.815566
246.997091	8000.052189	11.813530	-0.051706	4.815564
247.048356	8000.076547	11.818535	-0.051716	4.815571
247.035790	8000.066754	11.823539	-0.051714	4.815568
246.940952	8000.044938	11.828544	-0.051697	4.815562
247.136304	8000.093009	11.833549	-0.051733	4.815576
247.220509	8000.054894	11.838554	-0.051749	4.815564
247.164843	8000.076437	11.843559	-0.051739	4.815571
247.007645	8000.041855	11.848563	-0.051710	4.815561
247.123223	8000.029883	11.853568	-0.051732	4.815557
247.196419	8000.083435	11.858573	-0.051746	4.815572
247.166238	8000.039179	11.863578	-0.051741	4.815560
246.960276	8000.074288	11.868583	-0.051703	4.815571
247.037016	8000.080906	11.873587	-0.051717	4.815572
246.918990	8000.059780	11.878592	-0.051695	4.815567
247.075506	8000.087992	11.883597	-0.051725	4.815574
247.153185	8000.058314	11.888602	-0.051740	4.815565
247.249917	8000.071667	11.893607	-0.051758	4.815569
247.265113	8000.071940	11.898611	-0.051761	4.815569
247.062130	8000.049425	11.903616	-0.051724	4.815563
247.160961	8000.069220	11.908621	-0.051742	4.815568
246.993210	8000.055825	11.913626	-0.051711	4.815565
247.135644	8000.103032	11.918631	-0.051738	4.815578
247.294941	8000.085367	11.923635	-0.051768	4.815572
247.250086	8000.071843	11.928640	-0.051760	4.815569
247.172036	8000.096225	11.933645	-0.051746	4.815576
247.235573	8000.057771	11.938650	-0.051758	4.815565
247.394170	8000.060387	11.943655	-0.051788	4.815565
247.273303	8000.072321	11.948659	-0.051765	4.815569
247.128638	8000.049691	11.953664	-0.051739	4.815563
247.408250	8000.066031	11.958669	-0.051791	4.815566
247.312259	8000.036720	11.963674	-0.051773	4.815558
247.098293	8000.068494	11.968679	-0.051734	4.815568
247.167469	8000.042949	11.973683	-0.051747	4.815561
247.142471	8000.029749	11.978688	-0.051743	4.815557
247.265808	8000.069168	11.983693	-0.051766	4.815568
247.236289	8000.067643	11.988698	-0.051761	4.815567
247.100195	8000.073989	11.993703	-0.051736	4.815570
247.098273	8000.069710	11.998707	-0.051736	4.815569
247.143116	8000.080080	12.003712	-0.051744	4.815572
247.277507	8000.074823	12.008717	-0.051770	4.815569
247.193234	8000.065996	12.013722	-0.051754	4.815567
247.157567	8000.084662	12.018727	-0.051748	4.815573
247.225748	8000.081528	12.023731	-0.051761	4.815572
247.267484	8000.036311	12.028736	-0.051769	4.815558
247.379070	8000.079810	12.033741	-0.051790	4.815570
247.234742	8000.050778	12.038746	-0.051763	4.815562
247.452593	8000.085333	12.043751	-0.051804	4.815572
247.152502	8000.067640	12.048755	-0.051749	4.815568
246.941080	8000.053532	12.053760	-0.051709	4.815565
247.120721	8000.076782	12.058765	-0.051743	4.815571
247.262541	8000.052424	12.063770	-0.051770	4.815563
247.060640	8000.080123	12.068775	-0.051733	4.815572
247.115363	8000.082109	12.073779	-0.051743	4.815572
247.204116	8000.054748	12.078784	-0.051760	4.815564
247.276388	8000.073041	12.083789	-0.051774	4.815569
247.052488	8000.038437	12.088794	-0.051732	4.815560
247.241452	8000.055432	12.093799	-0.051768	4.815564
247.392983	8000.055796	12.098803	-0.051796	4.815563
247.116766	8000.028881	12.103808	-0.051745	4.815557
247.367220	8000.059696	12.108813	-0.051792	4.815564
247.318657	8000.035432	12.113818	-0.051783	4.815557
247.228369	8000.045730	12.118823	-0.051767	4.815561
247.347926	8000.064796	12.123827	-0.051789	4.815566
247.146680	8000.032697	12.128832	-0.051752	4.815557
247.196717	8000.048491	12.133837	-0.051762	4.815562
247.167049	8000.014924	12.138842	-0.051756	4.815552
247.096967	8000.038368	12.143847	-0.051744	4.815559
247.264729	8000.042201	12.148851	-0.051775	4.815560
247.005738	8000.056151	12.153856	-0.051727	4.815565
247.230434	8000.073730	12.158861	-0.051769	4.815569
247.197903	8000.057204	12.163866	-0.051764	4.815564
247.133112	8000.065782	12.168871	-0.051752	4.815567
247.155935	8000.065112	12.173875	-0.051756	4.815567
247.337102	8000.033919	12.178880	-0.051790	4.815557
247.505112	8000.079409	12.183885	-0.051822	4.815569
247.241139	8000.056966	12.188890	-0.051773	4.815564
247.064870	8000.044500	12.193895	-0.051740	4.815561
247.398111	8000.060647	12.198899	-0.051803	4.815564
247.254707	8000.066874	12.203904	-0.051776	4.815567
247.283682	8000.067372	12.208909	-0.051782	4.815567
247.286162	8000.048213	12.213914	-0.051783	4.815561
247.159932	8000.072876	12.218919	-0.051760	4.815569
247.279519	8000.075922	12.223923	-0.051782	4.815569
247.083429	8000.037500	12.228928	-0.051746	4.815559
247.323510	8000.083098	12.233933	-0.051791	4.815571
247.121171	8000.063798	12.238938	-0.051753	4.815567
247.208453	8000.082337	12.243943	-0.051770	4.815572
247.373970	8000.061569	12.248947	-0.051801	4.815565
247.185433	8000.043562	12.253952	-0.051766	4.815560
247.445023	8000.076663	12.258957	-0.051815	4.815569
247.418697	8000.038878	12.263962	-0.051810	4.815558
247.444884	8000.064962	12.268967	-0.051815	4.815565
247.198789	8000.054559	12.273971	-0.051770	4.815563
247.302253	8000.053070	12.278976	-0.051789	4.815562
247.537828	8000.083643	12.283981	-0.051834	4.815570
247.300187	8000.038134	12.288986	-0.051790	4.815558
247.249023	8000.075771	12.293991	-0.051780	4.815569
247.481402	8000.068912	12.298995	-0.051824	4.815566
247.390261	8000.016183	12.304000	-0.051807	4.815551
247.263743	8000.070746	12.309005	-0.051784	4.815568
247.242813	8000.048001	12.314010	-0.051780	4.815561
247.224829	8000.066956	12.319015	-0.051777	4.815567
247.250994	8000.054592	12.324019	-0.051782	4.815563
247.193972	8000.044073	12.329024	-0.051772	4.815560
247.336579	8000.057108	12.334029	-0.051799	4.815563
247.404314	8000.039015	12.339034	-0.051812	4.815558
247.445520	8000.070685	12.344039	-0.051820	4.815567
247.578732	8000.072886	12.349043	-0.051845	4.815567
247.433843	8000.054523	12.354048	-0.051818	4.815562
247.440008	8000.074941	12.359053	-0.051820	4.815568
247.520588	8000.069874	12.364058	-0.051835	4.815566
247.437448	8000.051453	12.369063	-0.051820	4.815561
247.657410	8000.059343	12.374067	-0.051861	4.815562
247.392520	8000.036884	12.379072	-0.051812	4.815557
247.444201	8000.084746	12.384077	-0.051822	4.815571
247.456377	8000.087105	12.389082	-0.051824	4.815572
247.067303	8000.073299	12.394087	-0.051752	4.815569
247.338887	8000.062808	12.399091	-0.051803	4.815565
247.273168	8000.052147	12.404096	-0.051791	4.815562
247.297013	8000.081397	12.409101	-0.051796	4.815571
247.359150	8000.046125	12.414106	-0.051808	4.815560
247.315646	8000.058255	12.419111	-0.051800	4.815564
247.329375	8000.065980	12.424115	-0.051803	4.815566
247.297379	8000.046258	12.429120	-0.051797	4.815560
247.454337	8000.083023	12.434125	-0.051827	4.815570
247.234143	8000.022847	12.439130	-0.051786	4.815554
247.280801	8000.046062	12.444135	-0.051795	4.815560
247.532562	8000.055539	12.449139	-0.051842	4.815562
247.577024	8000.055222	12.454144	-0.051850	4.815562
247.478694	8000.065389	12.459149	-0.051832	4.815565
247.557013	8000.039993	12.464154	-0.051847	4.815557
247.535084	8000.063156	12.469159	-0.051844	4.815564
247.426545	8000.071019	12.474163	-0.051824	4.815567
247.313585	8000.024343	12.479168	-0.051803	4.815554
247.584893	8000.077928	12.484173	-0.051854	4.815568
247.733292	8000.067561	12.489178	-0.051882	4.815564
247.429818	8000.080784	12.494183	-0.051825	4.815570
247.496416	8000.080829	12.499187	-0.051838	4.815569
247.583994	8000.052380	12.504192	-0.051855	4.815561
247.610915	8000.093429	12.509197	-0.051860	4.815572
247.583930	8000.049224	12.514202	-0.051855	4.815560
247.669573	8000.064533	12.519207	-0.051871	4.815564
247.727077	8000.072973	12.524211	-0.051882	4.815566
247.538454	8000.064576	12.529216	-0.051848	4.815564
247.644365	8000.074875	12.534221	-0.051868	4.815567
247.615490	8000.046660	12.539226	-0.051862	4.815559
247.640825	8000.077003	12.544231	-0.051867	4.815567
247.735700	8000.089258	12.549235	-0.051885	4.815571
247.505637	8000.041736	12.554240	-0.051843	4.815558
247.349798	8000.068051	12.559245	-0.051814	4.815566
247.417788	8000.052098	12.564250	-0.051827	4.815561
247.592983	8000.095570	12.569255	-0.051860	4.815573
247.485637	8000.091705	12.574259	-0.051840	4.815572
247.306340	8000.090937	12.579264	-0.051807	4.815573
247.628904	8000.103707	12.584269	-0.051868	4.815575
247.529065	8000.073264	12.589274	-0.051849	4.815567
247.494293	8000.090877	12.594279	-0.051843	4.815572
247.479272	8000.086385	12.599283	-0.051841	4.815571
247.563272	8000.054673	12.604288	-0.051856	4.815561
247.455889	8000.091392	12.609293	-0.051837	4.815572
247.570794	8000.084750	12.614298	-0.051858	4.815570
247.620963	8000.070642	12.619303	-0.051868	4.815566
247.723450	8000.086226	12.624307	-0.051887	4.815570
247.411204	8000.053381	12.629312	-0.051830	4.815562
247.458506	8000.057383	12.634317	-0.051839	4.815562
247.605031	8000.073685	12.639322	-0.051866	4.815567
247.496514	8000.082618	12.644327	-0.051846	4.815570
247.323437	8000.056319	12.649331	-0.051814	4.815563
247.326058	8000.078815	12.654336	-0.051815	4.815569
247.477882	8000.078115	12.659341	-0.051844	4.815568
247.565624	8000.040057	12.664346	-0.051860	4.815557
247.626376	8000.063503	12.669351	-0.051872	4.815563
247.719957	8000.063988	12.674355	-0.051890	4.815563
247.525162	8000.037335	12.679360	-0.051854	4.815556
247.430234	8000.078529	12.684365	-0.051836	4.815569
247.389346	8000.061866	12.689370	-0.051829	4.815564
247.634165	8000.056278	12.694375	-0.051875	4.815561
247.572402	8000.083062	12.699379	-0.051864	4.815569
247.471913	8000.029113	12.704384	-0.051845	4.815554
247.512942	8000.066120	12.709389	-0.051853	4.815565
247.434960	8000.041375	12.714394	-0.051839	4.815558
247.333179	8000.011969	12.719399	-0.051820	4.815550
247.464199	8000.049378	12.724403	-0.051845	4.815560
247.404797	8000.045228	12.729408	-0.051834	4.815559
247.552220	8000.074362	12.734413	-0.051862	4.815567
247.428748	8000.052077	12.739418	-0.051839	4.815561
247.383624	8000.055637	12.744423	-0.051831	4.815562
247.546522	8000.072207	12.749427	-0.051862	4.815566
247.584580	8000.037609	12.754432	-0.051869	4.815556
247.710042	8000.075996	12.759437	-0.051893	4.815567
247.678300	8000.065890	12.764442	-0.051887	4.815564
247.700944	8000.071625	12.769447	-0.051891	4.815565
247.694250	8000.045908	12.774451	-0.051890	4.815558
247.565449	8000.011788	12.779456	-0.051867	4.815548
247.519131	8000.064457	12.784461	-0.051858	4.815564
247.707728	8000.029114	12.789466	-0.051894	4.815553
247.673995	8000.026452	12.794471	-0.051888	4.815552
247.616679	8000.085349	12.799475	-0.051877	4.815570
247.563901	8000.037519	12.804480	-0.051868	4.815556
247.718026	8000.097735	12.809485	-0.051897	4.815573
247.732313	8000.080905	12.814490	-0.051900	4.815568
247.575231	8000.065547	12.819495	-0.051871	4.815564
247.730617	8000.057430	12.824499	-0.051900	4.815561
247.564512	8000.045129	12.829504	-0.051869	4.815558
247.670473	8000.086402	12.834509	-0.051889	4.815570
247.870895	8000.077953	12.839514	-0.051927	4.815566
247.643306	8000.072123	12.844519	-0.051885	4.815566
247.588410	8000.075523	12.849523	-0.051875	4.815567
247.712738	8000.063695	12.854528	-0.051898	4.815563
247.742328	8000.083428	12.859533	-0.051904	4.815568
247.511037	8000.057245	12.864538	-0.051861	4.815562
247.623438	8000.047358	12.869543	-0.051883	4.815558
247.714006	8000.085175	12.874547	-0.051900	4.815569
247.582163	8000.074502	12.879552	-0.051875	4.815567
247.662080	8000.086513	12.884557	-0.051891	4.815570
247.656749	8000.060818	12.889562	-0.051890	4.815562
247.559190	8000.030412	12.894567	-0.051872	4.815554
247.621046	8000.067760	12.899571	-0.051884	4.815564
247.599132	8000.056747	12.904576	-0.051880	4.815561
247.636674	8000.064861	12.909581	-0.051887	4.815563
247.669867	8000.050476	12.914586	-0.051894	4.815559
247.607924	8000.038809	12.919591	-0.051883	4.815556
247.592230	8000.077026	12.924595	-0.051880	4.815567
247.834433	8000.025471	12.929600	-0.051925	4.815551
247.689941	8000.080808	12.934605	-0.051899	4.815568
247.644438	8000.080089	12.939610	-0.051890	4.815568
247.740141	8000.043229	12.944615	-0.051909	4.815557
247.686589	8000.059467	12.949619	-0.051899	4.815562
247.607682	8000.059271	12.954624	-0.051884	4.815562
247.727107	8000.063383	12.959629	-0.051907	4.815562
247.545789	8000.063649	12.964634	-0.051874	4.815563
247.395642	8000.065493	12.969639	-0.051846	4.815565
247.498601	8000.066132	12.974643	-0.051865	4.815564
247.429847	8000.046877	12.979648	-0.051853	4.815559
247.491610	8000.073543	12.984653	-0.051865	4.815567
247.530297	8000.053908	12.989658	-0.051872	4.815561
247.528491	8000.053903	12.994663	-0.051872	4.815561
247.456287	8000.077313	12.999667	-0.051859	4.815568
247.621145	8000.072555	13.004672	-0.051890	4.815566
247.564940	8000.075933	13.009677	-0.051880	4.815567
247.607810	8000.043550	13.014682	-0.051888	4.815557
247.432660	8000.048189	13.019687	-0.051856	4.815559
247.578024	8000.036705	13.024691	-0.051883	4.815555
247.609997	8000.034048	13.029696	-0.051889	4.815554
247.577189	8000.066645	13.034701	-0.051883	4.815564
247.661268	8000.057364	13.039706	-0.051899	4.815561
247.599052	8000.026467	13.044711	-0.051888	4.815552
247.619020	8000.070607	13.049715	-0.051892	4.815565
247.681456	8000.062040	13.054720	-0.051904	4.815562
247.867182	8000.083256	13.059725	-0.051939	4.815567
247.586660	8000.065881	13.064730	-0.051887	4.815564
247.617271	8000.085630	13.069735	-0.051893	4.815569
247.914424	8000.097986	13.074739	-0.051948	4.815572
247.761301	8000.066672	13.079744	-0.051920	4.815563
247.581151	8000.062686	13.084749	-0.051887	4.815563
247.748588	8000.069718	13.089754	-0.051918	4.815564
247.813539	8000.046240	13.094759	-0.051931	4.815557
247.828802	8000.042242	13.099763	-0.051934	4.815556
247.674358	8000.058968	13.104768	-0.051905	4.815561
247.809622	8000.088971	13.109773	-0.051931	4.815569
247.729076	8000.048163	13.114778	-0.051916	4.815558
247.685901	8000.070979	13.119783	-0.051908	4.815565
247.798980	8000.062171	13.124787	-0.051930	4.815562
247.629009	8000.031650	13.129792	-0.051898	4.815553
247.648860	8000.078992	13.134797	-0.051902	4.815567
247.664060	8000.048293	13.139802	-0.051905	4.815558
247.750672	8000.041189	13.144807	-0.051922	4.815556
247.776579	8000.080086	13.149811	-0.051927	4.815567
247.705677	8000.068272	13.154816	-0.051914	4.815564
247.863110	8000.081549	13.159821	-0.051944	4.815567
247.772205	8000.066204	13.164826	-0.051927	4.815563
247.548998	8000.065786	13.169831	-0.051886	4.815564
247.795879	8000.077321	13.174835	-0.051932	4.815566
247.828627	8000.025548	13.179840	-0.051938	4.815551
247.772867	8000.043886	13.184845	-0.051928	4.815556
247.792303	8000.045296	13.189850	-0.051932	4.815557
247.914587	8000.025958	13.194855	-0.051955	4.815550
247.844479	8000.041926	13.199859	-0.051942	4.815555
247.829780	8000.027826	13.204864	-0.051940	4.815551
247.851885	8000.082682	13.209869	-0.051944	4.815567
247.992077	8000.066841	13.214874	-0.051971	4.815562
247.789955	8000.075311	13.219879	-0.051933	4.815565
247.728211	8000.081803	13.224883	-0.051922	4.815567
247.752523	8000.052321	13.229888	-0.051927	4.815559
247.762165	8000.074932	13.234893	-0.051929	4.815565
248.031179	8000.080420	13.239898	-0.051979	4.815566
247.804331	8000.087418	13.244903	-0.051937	4.815569
247.938007	8000.099240	13.249907	-0.051963	4.815572
247.727109	8000.077662	13.254912	-0.051924	4.815566
247.860678	8000.090550	13.259917	-0.051949	4.815569
247.893811	8000.078299	13.264922	-0.051955	4.815566
247.875886	8000.050263	13.269927	-0.051952	4.815557
248.080624	8000.081402	13.274931	-0.051991	4.815566
248.070023	8000.049212	13.279936	-0.051989	4.815556
247.954763	8000.083667	13.284941	-0.051968	4.815567
247.621795	8000.065435	13.289946	-0.051906	4.815563
247.565923	8000.056002	13.294951	-0.051896	4.815561
247.840875	8000.086152	13.299955	-0.051947	4.815568
247.663951	8000.043769	13.304960	-0.051915	4.815557
247.664252	8000.085452	13.309965	-0.051915	4.815569
247.830517	8000.067901	13.314970	-0.051946	4.815563
247.663439	8000.056652	13.319975	-0.051915	4.815560
247.725385	8000.083321	13.324979	-0.051927	4.815568
248.002040	8000.046213	13.329984	-0.051979	4.815556
248.024856	8000.070108	13.334989	-0.051984	4.815562
248.074617	8000.060265	13.339994	-0.051993	4.815559
248.103787	8000.065039	13.344999	-0.051999	4.815561
248.041350	8000.097153	13.350003	-0.051988	4.815570
247.714692	8000.050186	13.355008	-0.051927	4.815558
247.780306	8000.054487	13.360013	-0.051939	4.815559
248.001869	8000.068813	13.365018	-0.051981	4.815562
247.779474	8000.045979	13.370023	-0.051940	4.815557
247.536089	8000.062320	13.375027	-0.051895	4.815562
247.778344	8000.055623	13.380032	-0.051940	4.815559
247.845353	8000.080239	13.385037	-0.051953	4.815566
247.743835	8000.058312	13.390042	-0.051934	4.815560
247.761029	8000.063958	13.395047	-0.051938	4.815562
248.035428	8000.080215	13.400051	-0.051989	4.815565
247.669785	8000.026204	13.405056	-0.051921	4.815551
247.767164	8000.064133	13.410061	-0.051940	4.815562
248.062494	8000.065780	13.415066	-0.051995	4.815561
247.935696	8000.073345	13.420071	-0.051972	4.815564
247.882626	8000.101339	13.425075	-0.051962	4.815572
247.836312	8000.048274	13.430080	-0.051954	4.815557
247.728199	8000.076437	13.435085	-0.051934	4.815566
247.854889	8000.071055	13.440090	-0.051958	4.815563
247.884448	8000.046998	13.445095	-0.051964	4.815556
247.925717	8000.053038	13.450099	-0.051972	4.815558
247.814884	8000.050183	13.455104	-0.051951	4.815557
247.796267	8000.070197	13.460109	-0.051948	4.815563
247.918417	8000.059401	13.465114	-0.051971	4.815560
247.823785	8000.046131	13.470119	-0.051954	4.815556
247.804150	8000.050107	13.475123	-0.051950	4.815557
247.890975	8000.026986	13.480128	-0.051967	4.815550
247.968737	8000.063527	13.485133	-0.051982	4.815561
247.880556	8000.063178	13.490138	-0.051966	4.815561
247.865465	8000.056548	13.495143	-0.051963	4.815559
248.027879	8000.083792	13.500147	-0.051994	4.815566
247.879719	8000.056831	13.505152	-0.051966	4.815559
247.820232	8000.107149	13.510157	-0.051955	4.815574
247.806910	8000.058895	13.515162	-0.051953	4.815560
247.711627	8000.059499	13.520167	-0.051936	4.815561
247.688635	8000.057012	13.525171	-0.051932	4.815560
247.819980	8000.038890	13.530176	-0.051956	4.815554
247.879561	8000.090086	13.535181	-0.051968	4.815569
247.831447	8000.079712	13.540186	-0.051959	4.815566
247.638097	8000.052013	13.545191	-0.051923	4.815559
247.967524	8000.072373	13.550195	-0.051985	4.815563
247.844793	8000.047964	13.555200	-0.051963	4.815557
247.741886	8000.093301	13.560205	-0.051944	4.815570
248.032927	8000.092741	13.565210	-0.051998	4.815569
247.891691	8000.048805	13.570215	-0.051972	4.815557
247.828034	8000.062742	13.575219	-0.051961	4.815561
247.754243	8000.045540	13.580224	-0.051947	4.815556
247.966293	8000.090684	13.585229	-0.051987	4.815568
247.899171	8000.076795	13.590234	-0.051975	4.815565
247.889629	8000.056371	13.595239	-0.051973	4.815559
248.091889	8000.084266	13.600243	-0.052011	4.815566
247.761934	8000.021226	13.605248	-0.051950	4.815549
247.831178	8000.066171	13.610253	-0.051963	4.815562
247.929321	8000.035759	13.615258	-0.051982	4.815552
248.083509	8000.055391	13.620263	-0.052011	4.815557
248.090435	8000.075822	13.625267	-0.052012	4.815563
247.785644	8000.053778	13.630272	-0.051956	4.815558
248.137117	8000.070226	13.635277	-0.052021	4.815562
248.066256	8000.061617	13.640282	-0.052009	4.815559
247.864452	8000.024167	13.645287	-0.051971	4.815549
248.000483	8000.074476	13.650291	-0.051997	4.815563
247.989190	8000.052956	13.655296	-0.051995	4.815557
247.926020	8000.077581	13.660301	-0.051984	4.815565
248.034582	8000.094332	13.665306	-0.052004	4.815569
248.159782	8000.057954	13.670311	-0.052028	4.815558
248.210789	8000.088718	13.675315	-0.052037	4.815567
248.070034	8000.049061	13.680320	-0.052012	4.815556
247.990140	8000.099046	13.685325	-0.051997	4.815571
247.929511	8000.071379	13.690330	-0.051986	4.815563
247.960320	8000.042002	13.695335	-0.051992	4.815554
248.065648	8000.069381	13.700339	-0.052012	4.815562
248.081222	8000.058980	13.705344	-0.052015	4.815558
247.780401	8000.070109	13.710349	-0.051959	4.815563
247.962145	8000.053879	13.715354	-0.051993	4.815557
248.099512	8000.007019	13.720359	-0.052019	4.815543
248.063119	8000.075872	13.725363	-0.052013	4.815563
248.024967	8000.078477	13.730368	-0.052006	4.815564
248.041708	8000.078776	13.735373	-0.052009	4.815564
248.069527	8000.065371	13.740378	-0.052015	4.815560
247.861155	8000.055582	13.745383	-0.051976	4.815558
247.942700	8000.081504	13.750387	-0.051992	4.815566
247.873202	8000.050488	13.755392	-0.051979	4.815557
247.813348	8000.070896	13.760397	-0.051968	4.815563
247.971447	8000.080980	13.765402	-0.051998	4.815565
248.027993	8000.048820	13.770407	-0.052009	4.815556
247.981637	8000.089741	13.775411	-0.052000	4.815568
247.895081	8000.059514	13.780416	-0.051985	4.815559
248.097262	8000.072455	13.785421	-0.052023	4.815562
248.051390	8000.080275	13.790426	-0.052014	4.815565
247.718740	8000.038551	13.795431	-0.051953	4.815554
247.813159	8000.076431	13.800435	-0.051970	4.815565
247.957913	8000.067073	13.805440	-0.051998	4.815561
247.949165	8000.096860	13.810445	-0.051996	4.815570
247.942513	8000.074347	13.815450	-0.051995	4.815563
247.893171	8000.055409	13.820455	-0.051987	4.815558
248.053086	8000.078340	13.825459	-0.052017	4.815564
248.029439	8000.053414	13.830464	-0.052012	4.815557
247.958526	8000.074708	13.835469	-0.052000	4.815563
248.213715	8000.062883	13.840474	-0.052047	4.815559
248.111414	8000.069780	13.845479	-0.052029	4.815561
248.035089	8000.102735	13.850483	-0.052015	4.815571
247.939514	8000.059544	13.855488	-0.051997	4.815559
247.932528	8000.079747	13.860493	-0.051996	4.815565
248.041969	8000.062336	13.865498	-0.052017	4.815559
248.092329	8000.098429	13.870503	-0.052026	4.815570
248.077054	8000.076844	13.875507	-0.052024	4.815563
248.163015	8000.061185	13.880512	-0.052040	4.815558
248.098714	8000.071907	13.885517	-0.052028	4.815562
248.233420	8000.081610	13.890522	-0.052054	4.815564
248.109979	8000.058256	13.895527	-0.052031	4.815558
248.094973	8000.056968	13.900531	-0.052029	4.815557
248.162436	8000.057027	13.905536	-0.052041	4.815557
248.150275	8000.088894	13.910541	-0.052039	4.815567
247.987815	8000.083060	13.915546	-0.052010	4.815566
248.022871	8000.052685	13.920551	-0.052016	4.815557
248.079675	8000.066454	13.925555	-0.052027	4.815560
248.126169	8000.054422	13.930560	-0.052036	4.815557
248.078069	8000.069682	13.935565	-0.052027	4.815561
248.171991	8000.092602	13.940570	-0.052045	4.815567
248.100924	8000.038064	13.945575	-0.052032	4.815552
247.959223	8000.081698	13.950579	-0.052006	4.815565
247.835329	8000.045521	13.955584	-0.051983	4.815555
247.918131	8000.056512	13.960589	-0.051999	4.815558
248.100380	8000.038154	13.965594	-0.052033	4.815552
248.096883	8000.049870	13.970599	-0.052033	4.815555
248.127913	8000.062150	13.975603	-0.052039	4.815559
248.068923	8000.045191	13.980608	-0.052028	4.815554
248.050479	8000.083363	13.985613	-0.052025	4.815565
248.175971	8000.075827	13.990618	-0.052049	4.815562
248.080721	8000.059342	13.995623	-0.052031	4.815558
248.054540	8000.084572	14.000627	-0.052027	4.815566
248.120311	8000.058971	14.005632	-0.052039	4.815558
248.092705	8000.094858	14.010637	-0.052034	4.815568
248.183775	8000.086759	14.015642	-0.052052	4.815566
248.057489	8000.060155	14.020647	-0.052028	4.815558
248.160949	8000.089639	14.025651	-0.052048	4.815567
247.996858	8000.078438	14.030656	-0.052018	4.815564
248.115333	8000.084671	14.035661	-0.052040	4.815565
248.002164	8000.082846	14.040666	-0.052019	4.815565
248.082668	8000.039329	14.045671	-0.052035	4.815552
248.258601	8000.081747	14.050675	-0.052068	4.815564
248.012199	8000.031819	14.055680	-0.052022	4.815550
248.004019	8000.056275	14.060685	-0.052021	4.815557
248.270948	8000.058526	14.065690	-0.052071	4.815557
248.270332	8000.047861	14.070695	-0.052071	4.815554
248.504792	8000.075215	14.075699	-0.052115	4.815561
248.322991	8000.063724	14.080704	-0.052081	4.815558
248.459838	8000.075598	14.085709	-0.052107	4.815561
248.257761	8000.093680	14.090714	-0.052070	4.815567
248.097367	8000.059042	14.095719	-0.052040	4.815558
248.126406	8000.086243	14.100723	-0.052046	4.815566
248.110884	8000.045428	14.105728	-0.052043	4.815554
248.159601	8000.086835	14.110733	-0.052053	4.815566
248.230873	8000.106181	14.115738	-0.052066	4.815571
248.209591	8000.071681	14.120743	-0.052062	4.815561
248.260673	8000.118467	14.125747	-0.052072	4.815574
248.372737	8000.070125	14.130752	-0.052093	4.815560
248.364899	8000.087110	14.135757	-0.052092	4.815565
248.217401	8000.065500	14.140762	-0.052065	4.815559
248.148505	8000.071875	14.145767	-0.052052	4.815561
248.392568	8000.110066	14.150771	-0.052098	4.815571
248.289638	8000.072095	14.155776	-0.052079	4.815561
248.356936	8000.089240	14.160781	-0.052092	4.815565
248.315539	8000.075772	14.165786	-0.052085	4.815562
247.940492	8000.051510	14.170791	-0.052015	4.815556
248.113561	8000.081065	14.175795	-0.052048	4.815564
248.072437	8000.079349	14.180800	-0.052040	4.815564
247.993643	8000.091971	14.185805	-0.052026	4.815568
248.286069	8000.107456	14.190810	-0.052081	4.815571
248.165688	8000.070267	14.195815	-0.052058	4.815561
248.302999	7999.186083	14.200819	-0.052084	4.815301

248.312884	7995.965532	14.205824	-0.052084	4.814360
248.139810	7990.541481	14.210829	-0.052048	4.812775
248.233094	7983.972193	14.215834	-0.052062	4.810852
248.068820	7976.572739	14.220839	-0.052027	4.808688
248.092836	7969.000526	14.225843	-0.052026	4.806470
248.171352	7961.179052	14.230848	-0.052036	4.804179
248.027186	7953.394111	14.235853	-0.052005	4.801898
248.012489	7945.355140	14.240858	-0.051997	4.799541
248.118647	7937.465560	14.245863	-0.052012	4.797226
248.266371	7929.399578	14.250867	-0.052034	4.794858
248.014259	7921.407226	14.255872	-0.051982	4.792512
247.843915	7913.309568	14.260877	-0.051946	4.790133
247.907624	7905.407243	14.265882	-0.051953	4.787810
247.804952	7897.331310	14.270887	-0.051929	4.785436
247.846770	7889.418407	14.275891	-0.051931	4.783107
247.621242	7881.428346	14.280896	-0.051885	4.780756
247.487002	7873.396892	14.285901	-0.051855	4.778391
247.558884	7865.397593	14.290906	-0.051863	4.776034
247.671580	7857.346638	14.295911	-0.051879	4.773660
247.405826	7849.419714	14.300915	-0.051825	4.771323
247.428330	7841.358660	14.305920	-0.051824	4.768944
247.752765	7833.381459	14.310925	-0.051879	4.766587
247.512031	7825.334672	14.315930	-0.051830	4.764211
247.361055	7817.421913	14.320935	-0.051797	4.761873
247.336970	7809.393204	14.325939	-0.051787	4.759499
247.425959	7801.416243	14.330944	-0.051799	4.757139
247.269226	7793.359233	14.335949	-0.051765	4.754755
247.247120	7785.326803	14.340954	-0.051756	4.752376
247.175565	7777.319993	14.345959	-0.051737	4.750004
247.096784	7769.297135	14.350963	-0.051718	4.747626
246.946543	7761.316518	14.355968	-0.051685	4.745259
247.219309	7753.348541	14.360973	-0.051731	4.742894
247.264679	7745.333768	14.365978	-0.051734	4.740515
247.069565	7737.359489	14.370983	-0.051693	4.738146
247.178257	7729.307181	14.375987	-0.051708	4.735753
246.936927	7721.325883	14.380992	-0.051658	4.733381
246.844749	7713.268252	14.385997	-0.051636	4.730984
246.784655	7705.310472	14.391002	-0.051620	4.728616
246.699235	7697.283112	14.396007	-0.051599	4.726225
246.895857	7689.295865	14.401011	-0.051631	4.723845
246.867616	7681.369273	14.406016	-0.051621	4.721482
246.818954	7673.304163	14.411021	-0.051607	4.719077
246.992188	7665.382050	14.416026	-0.051634	4.716713
246.548002	7657.296829	14.421031	-0.051547	4.714300
246.718062	7649.308527	14.426035	-0.051573	4.711914
246.733824	7641.287522	14.431040	-0.051571	4.709517
246.498462	7633.292738	14.436045	-0.051523	4.707127
246.646171	7625.275683	14.441050	-0.051545	4.704728
246.462805	7617.290567	14.446055	-0.051506	4.702339
246.527665	7609.329017	14.451059	-0.051513	4.699954
246.424147	7601.352652	14.456064	-0.051489	4.697565
246.436549	7593.243706	14.461069	-0.051486	4.695134
246.532055	7585.268531	14.466074	-0.051499	4.692742
246.302230	7577.248600	14.471079	-0.051451	4.690336
246.254773	7569.280741	14.476083	-0.051438	4.687944
246.391755	7561.267116	14.481088	-0.051458	4.685536
246.146602	7553.292840	14.486093	-0.051408	4.683140
246.137236	7545.347879	14.491098	-0.051401	4.680751
246.248520	7537.281034	14.496103	-0.051417	4.678324
246.151978	7529.295083	14.501107	-0.051394	4.675921
246.016795	7521.211532	14.506112	-0.051364	4.673486
245.932302	7513.113838	14.511117	-0.051343	4.671047
246.050067	7505.194197	14.516122	-0.051360	4.668659
245.785031	7497.211782	14.521127	-0.051306	4.666251
245.717275	7489.212661	14.526131	-0.051288	4.663837
245.641502	7481.243528	14.531136	-0.051269	4.661431
245.801107	7473.218435	14.536141	-0.051294	4.659007
245.758928	7465.291782	14.541146	-0.051281	4.656611
245.659565	7457.198754	14.546151	-0.051258	4.654164
245.878266	7449.235804	14.551155	-0.051294	4.651754
245.689305	7441.179871	14.556160	-0.051253	4.649316
245.661003	7433.240989	14.561165	-0.051243	4.646911
245.565416	7425.191748	14.566170	-0.051221	4.644472
245.429510	7417.254777	14.571175	-0.051190	4.642065
245.544834	7409.216522	14.576179	-0.051207	4.639627
245.526353	7401.270644	14.581184	-0.051199	4.637215
245.306525	7393.193944	14.586189	-0.051153	4.634762
245.410423	7385.186800	14.591194	-0.051167	4.632329
245.346786	7377.133310	14.596199	-0.051150	4.629881
245.284941	7369.196991	14.601203	-0.051134	4.627467
244.966827	7361.207186	14.606208	-0.051070	4.625036
244.962541	7353.165549	14.611213	-0.051064	4.622587
245.102461	7345.173333	14.616218	-0.051085	4.620152
244.989123	7337.188280	14.621223	-0.051059	4.617718
245.039111	7329.171685	14.626227	-0.051063	4.615273
245.122617	7321.181828	14.631232	-0.051074	4.612836
245.265198	7313.125611	14.636237	-0.051096	4.610376
245.190401	7305.176952	14.641242	-0.051077	4.607948
245.101719	7297.138572	14.646247	-0.051055	4.605491
245.224415	7289.187019	14.651251	-0.051073	4.603060
244.907030	7281.191125	14.656256	-0.051009	4.600614
244.673960	7273.185234	14.661261	-0.050961	4.598163
244.711940	7265.215929	14.666266	-0.050963	4.595722
244.902207	7257.128377	14.671271	-0.050993	4.593244
244.653726	7249.086647	14.676275	-0.050942	4.590778
244.719718	7241.115856	14.681280	-0.050950	4.588333
244.792954	7233.096401	14.686285	-0.050958	4.585871
244.641073	7225.142755	14.691290	-0.050925	4.583429
244.493576	7217.141599	14.696295	-0.050893	4.580970
244.610333	7209.120712	14.701299	-0.050910	4.578504
244.374281	7201.150827	14.706304	-0.050861	4.576053
244.289265	7193.112827	14.711309	-0.050840	4.573579
244.295000	7185.112358	14.716314	-0.050836	4.571115
244.236630	7177.096176	14.721319	-0.050820	4.568645
244.164037	7169.139088	14.726323	-0.050802	4.566192
244.112572	7161.111344	14.731328	-0.050787	4.563716
244.174049	7153.165392	14.736333	-0.050794	4.561264
244.167501	7145.118864	14.741338	-0.050788	4.558780
243.904545	7137.170847	14.746343	-0.050734	4.556324
244.084333	7129.113043	14.751347	-0.050762	4.553834
244.008581	7121.115343	14.756352	-0.050743	4.551360
243.883614	7113.054701	14.761357	-0.050715	4.548866
243.967319	7105.157714	14.766362	-0.050726	4.546421
243.810318	7097.094993	14.771367	-0.050692	4.543923
243.841644	7089.148483	14.776371	-0.050692	4.541460
243.788529	7081.135320	14.781376	-0.050678	4.538975
243.746045	7073.168757	14.786381	-0.050665	4.536503
243.694301	7065.123176	14.791386	-0.050650	4.534005
243.740916	7057.067352	14.796391	-0.050654	4.531503
243.598076	7049.090540	14.801395	-0.050622	4.529023
243.497737	7041.133927	14.806400	-0.050599	4.526549
243.410163	7033.093348	14.811405	-0.050578	4.524047
243.637192	7025.146208	14.816410	-0.050615	4.521573
243.563336	7017.093353	14.821415	-0.050596	4.519065
243.392469	7009.159912	14.826419	-0.050560	4.516592
243.508082	7001.076509	14.831424	-0.050576	4.514071
243.459568	6993.013907	14.836429	-0.050562	4.511556
243.375548	6985.058098	14.841434	-0.050542	4.509072
243.167901	6977.041805	14.846439	-0.050498	4.506567
243.189272	6969.065036	14.851443	-0.050497	4.504074
243.140708	6961.121245	14.856448	-0.050483	4.501590
243.109874	6953.060004	14.861453	-0.050472	4.499068
243.201080	6945.100885	14.866458	-0.050484	4.496577
243.105575	6937.058221	14.871463	-0.050462	4.494057
243.032168	6929.086624	14.876467	-0.050443	4.491559
243.153838	6921.024033	14.881472	-0.050461	4.489031
243.064747	6913.027730	14.886477	-0.050439	4.486521
242.982836	6905.060725	14.891482	-0.050419	4.484020
242.811951	6897.110057	14.896487	-0.050382	4.481522
243.021656	6889.082420	14.901491	-0.050416	4.479000
243.090805	6881.115330	14.906496	-0.050424	4.476495
242.566592	6873.012358	14.911501	-0.050322	4.473944
242.784201	6865.031873	14.916506	-0.050357	4.471432
242.887777	6857.034296	14.921511	-0.050372	4.468913
242.586327	6849.029025	14.926515	-0.050311	4.466389
242.291955	6841.007539	14.931520	-0.050251	4.463858
242.447450	6833.033838	14.936525	-0.050275	4.461343
242.463454	6825.018816	14.941530	-0.050273	4.458812
242.183718	6817.029765	14.946535	-0.050216	4.456288
242.244563	6809.032219	14.951539	-0.050222	4.453760
242.316549	6801.033135	14.956544	-0.050231	4.451231
242.248057	6792.982191	14.961549	-0.050213	4.448683
242.335697	6785.031445	14.966554	-0.050225	4.446166
242.209290	6777.000329	14.971559	-0.050196	4.443621
242.374320	6769.012290	14.976563	-0.050222	4.441090
242.015487	6761.031961	14.981568	-0.050150	4.438557
242.221728	6753.043596	14.986573	-0.050184	4.436023
242.290967	6745.028225	14.991578	-0.050192	4.433478
242.109907	6736.953213	14.996583	-0.050153	4.430912
242.046874	6728.951947	15.001587	-0.050136	4.428368
242.017354	6720.971503	15.006592	-0.050126	4.425830
241.644323	6712.968381	15.011597	-0.050051	4.423281
241.804022	6705.028682	15.016602	-0.050076	4.420753
241.749925	6696.974273	15.021607	-0.050061	4.418187
241.831745	6688.994927	15.026611	-0.050072	4.415643
241.752840	6680.992326	15.031616	-0.050052	4.413090
241.441712	6672.945258	15.036621	-0.049989	4.410520
241.741594	6664.991954	15.041626	-0.050040	4.407982
241.556746	6656.965984	15.046631	-0.050001	4.405416
241.524659	6649.015482	15.051635	-0.049990	4.402874
241.701511	6641.010525	15.056640	-0.050018	4.400314
241.539242	6632.993419	15.061645	-0.049983	4.397746
241.441377	6625.033568	15.066650	-0.049959	4.395196
241.454046	6616.968391	15.071655	-0.049957	4.392612
241.544356	6608.958202	15.076659	-0.049969	4.390043
241.254579	6601.001158	15.081664	-0.049910	4.387489
241.402606	6592.968205	15.086669	-0.049932	4.384911
241.350401	6585.009578	15.091674	-0.049918	4.382354
241.083779	6576.978912	15.096679	-0.049863	4.379771
241.119231	6569.013559	15.101683	-0.049865	4.377209
241.298934	6560.994914	15.106688	-0.049893	4.374630
241.180689	6552.989408	15.111693	-0.049867	4.372051
240.947097	6544.983107	15.116698	-0.049818	4.369470
240.967196	6536.972926	15.121703	-0.049817	4.366888
240.926265	6528.996718	15.126707	-0.049804	4.364315
240.805356	6521.049034	15.131712	-0.049777	4.361749
240.921599	6512.965159	15.136717	-0.049794	4.359139
241.055262	6505.031581	15.141722	-0.049814	4.356576
240.901305	6496.997383	15.146727	-0.049780	4.353977
240.689662	6488.872751	15.151731	-0.049736	4.351347
240.657525	6480.906604	15.156736	-0.049725	4.348768
240.482317	6472.918284	15.161741	-0.049687	4.346180
240.656103	6464.995906	15.166746	-0.049715	4.343613
240.371949	6456.974208	15.171751	-0.049657	4.341010
240.383753	6448.976176	15.176755	-0.049654	4.338414
240.302347	6440.984926	15.181760	-0.049634	4.335819
240.318610	6432.970455	15.186765	-0.049632	4.333215
240.503818	6424.928321	15.191770	-0.049662	4.330602
240.342636	6416.952317	15.196775	-0.049627	4.328006
240.179540	6408.962034	15.201779	-0.049591	4.325405
240.273130	6400.980474	15.206784	-0.049604	4.322806
240.250588	6392.945008	15.211789	-0.049595	4.320187
240.280097	6385.030978	15.216794	-0.049595	4.317607
240.266618	6376.928473	15.221799	-0.049588	4.314963
240.295624	6368.956156	15.226803	-0.049588	4.312361
240.286663	6360.910232	15.231808	-0.049582	4.309732
240.113191	6352.935163	15.236813	-0.049544	4.307124
240.144212	6344.925798	15.241818	-0.049545	4.304505
239.921701	6336.956928	15.246823	-0.049499	4.301895
239.855414	6328.927275	15.251827	-0.049482	4.299265
239.816510	6320.993344	15.256832	-0.049470	4.296665
239.799296	6312.902832	15.261837	-0.049461	4.294012
239.835122	6304.957773	15.266842	-0.049463	4.291406
239.649200	6296.894699	15.271847	-0.049423	4.288758
239.738975	6288.955197	15.276851	-0.049435	4.286150
239.763736	6280.960416	15.281856	-0.049435	4.283523
239.469833	6272.939742	15.286861	-0.049375	4.280883
239.455356	6264.957755	15.291866	-0.049368	4.278256
239.383843	6256.924342	15.296871	-0.049349	4.275610
239.450071	6248.908453	15.301875	-0.049357	4.272969
239.406472	6240.878608	15.306880	-0.049344	4.270322
239.429676	6232.909712	15.311885	-0.049343	4.267693
239.490043	6224.884224	15.316890	-0.049349	4.265044
239.327804	6216.873454	15.321895	-0.049314	4.262397
239.379457	6208.882731	15.326899	-0.049319	4.259756
239.415815	6200.950213	15.331904	-0.049321	4.257133
239.221076	6192.891212	15.336909	-0.049280	4.254464
239.333210	6184.903346	15.341914	-0.049296	4.251820
239.069929	6176.906351	15.346919	-0.049242	4.249168
239.090643	6168.914989	15.351923	-0.049241	4.246519
239.174677	6160.954112	15.356928	-0.049251	4.243878
239.073291	6152.915045	15.361933	-0.049228	4.241209
239.149315	6144.974677	15.366938	-0.049237	4.238572
238.902491	6136.961182	15.371943	-0.049186	4.235906
238.801910	6128.939223	15.376947	-0.049162	4.233237
238.815226	6120.905923	15.381952	-0.049160	4.230564
238.821129	6112.902288	15.386957	-0.049156	4.227898
238.845496	6104.900349	15.391962	-0.049156	4.225232
238.888707	6096.948763	15.396967	-0.049159	4.222581
238.574734	6088.943623	15.401971	-0.049095	4.219907
238.608343	6080.973424	15.406976	-0.049097	4.217247
238.803617	6072.929546	15.411981	-0.049128	4.214562
238.551965	6064.933293	15.416986	-0.049076	4.211886
238.371391	6056.921388	15.421991	-0.049038	4.209204
238.391202	6048.933658	15.426995	-0.049036	4.206531
238.437845	6040.929670	15.432000	-0.049040	4.203851
238.138254	6032.947189	15.437005	-0.048979	4.201172
238.275130	6024.956195	15.442010	-0.049000	4.198494
238.379457	6016.953611	15.447015	-0.049015	4.195810
238.347330	6008.864724	15.452019	-0.049004	4.193093
238.275036	6000.837188	15.457024	-0.048985	4.190395
238.348273	5992.839873	15.462029	-0.048994	4.187707
238.499065	5984.862780	15.467034	-0.049017	4.185025
238.222183	5976.956614	15.472039	-0.048961	4.182360
238.105436	5968.890072	15.477043	-0.048934	4.179642
238.061529	5960.985678	15.482048	-0.048921	4.176977
237.884190	5952.895550	15.487053	-0.048883	4.174246
237.860264	5944.903687	15.492058	-0.048873	4.171548
237.804540	5936.894978	15.497063	-0.048858	4.168843
237.907072	5928.896308	15.502067	-0.048872	4.166141
237.908055	5920.921009	15.507072	-0.048868	4.163444
237.722756	5912.926816	15.512077	-0.048828	4.160736
237.643762	5904.964670	15.517082	-0.048809	4.158039
237.409376	5896.900731	15.522087	-0.048760	4.155304
237.580381	5888.904513	15.527091	-0.048787	4.152595
237.546970	5880.875522	15.532096	-0.048776	4.149870
237.303364	5872.878516	15.537101	-0.048725	4.147152
237.479850	5864.865584	15.542106	-0.048753	4.144432
237.550910	5856.913921	15.547111	-0.048762	4.141729
237.460560	5848.880531	15.552115	-0.048740	4.138995
237.207256	5840.944527	15.557120	-0.048688	4.136291
237.183686	5832.873593	15.562125	-0.048678	4.133541
237.381127	5824.884259	15.567130	-0.048710	4.130820
237.230373	5816.878052	15.572135	-0.048677	4.128088
237.302778	5808.886401	15.577139	-0.048686	4.125361
237.059030	5800.937258	15.582144	-0.048636	4.122643
236.976886	5792.887023	15.587149	-0.048615	4.119891
236.911153	5784.961142	15.592154	-0.048598	4.117179
236.765874	5776.917647	15.597159	-0.048566	4.114425
236.651309	5768.893941	15.602163	-0.048540	4.111675
236.700334	5760.890410	15.607168	-0.048544	4.108933
236.694521	5752.843328	15.612173	-0.048538	4.106174
236.798630	5744.902965	15.617178	-0.048552	4.103450
236.758075	5736.894322	15.622183	-0.048540	4.100700
236.640120	5728.925856	15.627187	-0.048513	4.097960
236.958870	5720.918591	15.632192	-0.048568	4.095212
236.607984	5712.898255	15.637197	-0.048497	4.092447
236.542605	5704.878641	15.642202	-0.048480	4.089685
236.530740	5696.906757	15.647207	-0.048473	4.086939
236.627141	5688.907895	15.652211	-0.048486	4.084182
236.613558	5680.977576	15.657216	-0.048479	4.081446
236.501042	5672.937213	15.662221	-0.048453	4.078669
236.624997	5664.970573	15.667226	-0.048471	4.075918
236.460620	5656.956806	15.672231	-0.048435	4.073146
236.270204	5648.912639	15.677235	-0.048395	4.070360
236.389967	5640.930841	15.682240	-0.048412	4.067599
236.170799	5632.934965	15.687245	-0.048367	4.064826
236.189179	5624.974484	15.692250	-0.048365	4.062066
236.076747	5616.947444	15.697255	-0.048339	4.059280
236.160596	5608.987046	15.702259	-0.048350	4.056518
236.152470	5600.942438	15.707264	-0.048343	4.053724
236.203734	5592.838051	15.712269	-0.048348	4.050907
236.140160	5584.916386	15.717274	-0.048331	4.048151
235.892758	5576.933507	15.722279	-0.048280	4.045369
235.862022	5568.993613	15.727283	-0.048270	4.042603
235.900569	5560.974738	15.732288	-0.048272	4.039808
235.863105	5552.973608	15.737293	-0.048260	4.037017
235.735336	5544.964937	15.742298	-0.048231	4.034219
235.602394	5536.839695	15.747303	-0.048201	4.031379
235.608196	5528.865106	15.752307	-0.048198	4.028592
235.653439	5520.916624	15.757312	-0.048201	4.025813
235.382036	5512.919740	15.762317	-0.048146	4.023009
235.631845	5504.916286	15.767322	-0.048187	4.020210
235.484599	5496.933202	15.772327	-0.048155	4.017409
235.223766	5488.925210	15.777331	-0.048101	4.014596
235.228556	5480.910204	15.782336	-0.048097	4.011783
235.257371	5472.887308	15.787341	-0.048098	4.008966
235.428348	5464.929352	15.792346	-0.048125	4.006171
235.219744	5456.916850	15.797351	-0.048081	4.003349
235.224353	5448.886226	15.802355	-0.048077	4.000523
235.268620	5440.947189	15.807360	-0.048080	3.997727
235.380257	5432.959257	15.812365	-0.048096	3.994913
235.224039	5424.942336	15.817370	-0.048062	3.992083
235.212055	5416.876770	15.822375	-0.048055	3.989235
234.936043	5408.946721	15.827379	-0.047999	3.986430
234.954005	5400.955718	15.832384	-0.047997	3.983605
234.882491	5392.952508	15.837389	-0.047979	3.980773
234.676500	5384.971923	15.842394	-0.047935	3.977944
234.672283	5376.977906	15.847399	-0.047930	3.975112
235.047619	5368.903841	15.852403	-0.047995	3.972256
234.879363	5360.943080	15.857408	-0.047958	3.969429
234.730547	5352.951976	15.862413	-0.047926	3.966590
234.758034	5344.979299	15.867418	-0.047926	3.963758
234.786774	5336.992943	15.872423	-0.047926	3.960919
234.675525	5329.002400	15.877427	-0.047901	3.958074
234.558822	5321.020550	15.882432	-0.047874	3.955231
234.625255	5312.946237	15.887437	-0.047882	3.952355
234.316626	5304.963508	15.892442	-0.047819	3.949503
234.226834	5296.995184	15.897447	-0.047798	3.946658
234.326643	5288.973489	15.902451	-0.047811	3.943796
234.196182	5281.000414	15.907456	-0.047782	3.940945
234.103566	5273.015583	15.912461	-0.047760	3.938088
234.252542	5265.033269	15.917466	-0.047783	3.935234
234.180861	5256.995399	15.922471	-0.047764	3.932354
234.115137	5248.939642	15.927475	-0.047747	3.929466
234.025688	5241.015475	15.932480	-0.047726	3.926622
234.035982	5232.977262	15.937485	-0.047723	3.923738
234.175940	5225.019183	15.942490	-0.047744	3.920882
233.920079	5217.020181	15.947495	-0.047691	3.918002
234.183209	5209.005807	15.952499	-0.047735	3.915124
234.160319	5200.987645	15.957504	-0.047726	3.912238
233.916752	5192.941750	15.962509	-0.047676	3.909335
233.961741	5185.013394	15.967514	-0.047679	3.906478
233.849098	5176.979637	15.972519	-0.047653	3.903577
233.754357	5169.010618	15.977523	-0.047631	3.900699
233.680860	5161.049870	15.982528	-0.047612	3.897821
233.686981	5153.006266	15.987533	-0.047608	3.894913
233.811647	5144.993469	15.992538	-0.047627	3.892016
233.557856	5136.972154	15.997543	-0.047574	3.889107
233.492109	5129.020167	16.002547	-0.047557	3.886224
233.529843	5121.009217	16.007552	-0.047559	3.883319
233.436512	5112.988907	16.012557	-0.047537	3.880407
233.451184	5105.054790	16.017562	-0.047535	3.877525
233.550679	5097.018103	16.022567	-0.047548	3.874606
233.360663	5088.769732	16.027571	-0.047508	3.871602
233.370296	5080.883081	16.032576	-0.047505	3.868732
233.235336	5072.892800	16.037581	-0.047475	3.865818
233.218692	5064.968907	16.042586	-0.047467	3.862929
233.034971	5056.972874	16.047591	-0.047428	3.860008
233.092169	5048.991933	16.052595	-0.047433	3.857095
233.284089	5040.993330	16.057600	-0.047464	3.854177
232.855757	5032.989022	16.062605	-0.047380	3.851241
233.088199	5025.014782	16.067610	-0.047418	3.848328
233.146006	5016.987215	16.072615	-0.047424	3.845389
232.891458	5009.054796	16.077619	-0.047371	3.842476
232.640990	5001.101901	16.082624	-0.047320	3.839554
232.571011	4993.071874	16.087629	-0.047302	3.836605
232.603093	4985.073711	16.092634	-0.047303	3.833668
232.549594	4977.035600	16.097639	-0.047288	3.830711
232.568980	4969.012291	16.102643	-0.047287	3.827760
232.483619	4961.057947	16.107648	-0.047266	3.824829
232.531153	4953.046219	16.112653	-0.047270	3.821878
232.611013	4945.080269	16.117658	-0.047280	3.818942
232.564124	4937.092225	16.122663	-0.047266	3.815993
232.379614	4929.089632	16.127667	-0.047227	3.813033
232.327120	4921.071307	16.132672	-0.047212	3.810068
232.509871	4913.080112	16.137677	-0.047241	3.807116
232.598548	4905.080319	16.142682	-0.047253	3.804157
232.417563	4897.178370	16.147687	-0.047214	3.801225
232.250646	4889.126905	16.152691	-0.047178	3.798236
232.519553	4881.138502	16.157696	-0.047223	3.795278
232.287747	4873.078360	16.162701	-0.047175	3.792279
232.238877	4865.057473	16.167706	-0.047161	3.789297
232.218694	4857.089039	16.172711	-0.047152	3.786333
232.006537	4849.066262	16.177715	-0.047108	3.783342
231.969592	4841.111438	16.182720	-0.047096	3.780377
231.861911	4833.134496	16.187725	-0.047071	3.777401
231.968588	4825.111619	16.192730	-0.047086	3.774409
231.963407	4817.108535	16.197735	-0.047080	3.771421
231.939154	4809.067872	16.202739	-0.047071	3.768415
231.891525	4801.141867	16.207744	-0.047057	3.765450
231.546179	4793.140326	16.212749	-0.046988	3.762447
231.636822	4785.132698	16.217754	-0.047000	3.759449
231.664925	4777.178561	16.222759	-0.047000	3.756467
231.756478	4769.090410	16.227763	-0.047012	3.753435
231.499801	4761.122609	16.232768	-0.046959	3.750437
231.323454	4753.130556	16.237773	-0.046922	3.747429
231.534840	4745.086781	16.242778	-0.046956	3.744408
231.352474	4737.175207	16.247783	-0.046917	3.741426
231.284808	4729.127800	16.252787	-0.046900	3.738392
231.370596	4721.167509	16.257792	-0.046911	3.735393
231.425613	4713.136130	16.262797	-0.046916	3.732364
231.317612	4705.130677	16.267802	-0.046891	3.729338
231.224617	4697.194396	16.272807	-0.046869	3.726336
231.258835	4689.162393	16.277811	-0.046870	3.723299
231.230538	4681.214300	16.282816	-0.046860	3.720289
231.104617	4673.216321	16.287821	-0.046832	3.717256
231.127455	4665.202190	16.292826	-0.046831	3.714218
231.041460	4657.099672	16.297831	-0.046810	3.711141
231.148712	4649.122044	16.302835	-0.046825	3.708113
231.102725	4641.168229	16.307840	-0.046812	3.705089
230.831374	4633.201161	16.312845	-0.046756	3.702051
230.694045	4625.199218	16.317850	-0.046726	3.699001
230.715117	4617.225501	16.322855	-0.046725	3.695963
230.741431	4609.213807	16.327859	-0.046725	3.692908
230.556713	4601.240630	16.332864	-0.046685	3.689860
230.693005	4593.214517	16.337869	-0.046706	3.686797
230.789158	4585.234409	16.342874	-0.046719	3.683748
230.567354	4577.265697	16.347879	-0.046673	3.680694
230.391252	4569.278657	16.352883	-0.046635	3.677630
230.506260	4561.278074	16.357888	-0.046651	3.674567
230.472278	4553.217642	16.362893	-0.046640	3.671474
230.539771	4545.214907	16.367898	-0.046648	3.668403
230.389368	4537.250600	16.372903	-0.046615	3.665339
230.312967	4529.266110	16.377907	-0.046596	3.662266
230.341219	4521.247210	16.382912	-0.046596	3.659180
230.207857	4513.271983	16.387917	-0.046566	3.656104
230.189882	4505.264094	16.392922	-0.046558	3.653016
230.204360	4497.235700	16.397927	-0.046556	3.649919
229.880548	4489.272075	16.402931	-0.046490	3.646834
230.032831	4481.288230	16.407936	-0.046514	3.643752
229.962074	4473.278068	16.412941	-0.046496	3.640652
230.013142	4465.319531	16.417946	-0.046500	3.637571
229.940925	4457.315071	16.422951	-0.046482	3.634468
229.752265	4449.255591	16.427955	-0.046442	3.631337
229.741314	4441.276768	16.432960	-0.046435	3.628239
229.635295	4433.259213	16.437965	-0.046410	3.625121
229.803299	4425.289570	16.442970	-0.046437	3.622026
229.699816	4417.303272	16.447975	-0.046412	3.618915
229.508682	4409.329275	16.452979	-0.046372	3.615804
229.799837	4401.316911	16.457984	-0.046421	3.612688
229.613770	4393.287602	16.462989	-0.046382	3.609550
229.511232	4385.345720	16.467994	-0.046358	3.606445
229.345059	4377.358583	16.472999	-0.046322	3.603319
229.446913	4369.351316	16.478003	-0.046336	3.600189
229.406483	4361.426523	16.483008	-0.046323	3.597085
229.130716	4353.396520	16.488013	-0.046267	3.593930
229.252545	4345.363331	16.493018	-0.046285	3.590782
229.221030	4337.399092	16.498023	-0.046274	3.587655
229.153842	4329.364987	16.503027	-0.046257	3.584496
229.096919	4321.429294	16.508032	-0.046241	3.581373
229.170890	4313.424423	16.513037	-0.046250	3.578224
229.138750	4305.436699	16.518042	-0.046239	3.575076
229.210533	4297.405683	16.523047	-0.046247	3.571912
229.167628	4289.387017	16.528051	-0.046234	3.568746
228.981327	4281.439769	16.533056	-0.046195	3.565601
228.764528	4273.463198	16.538061	-0.046150	3.562441
228.892551	4265.464341	16.543066	-0.046169	3.559279
228.897145	4257.490364	16.548071	-0.046164	3.556121
228.792213	4249.393873	16.553075	-0.046140	3.552908
228.813312	4241.352765	16.558080	-0.046139	3.549718
228.772377	4233.362808	16.563085	-0.046126	3.546544
228.813405	4225.406067	16.568090	-0.046129	3.543382
228.590255	4217.455099	16.573095	-0.046083	3.540212
228.672390	4209.453085	16.578099	-0.046093	3.537028
228.676908	4201.448451	16.583104	-0.046089	3.533837
228.419585	4193.440381	16.588109	-0.046036	3.530635
228.260218	4185.477585	16.593114	-0.046001	3.527450
228.426216	4177.437159	16.598119	-0.046027	3.524242
228.233915	4169.512466	16.603123	-0.045987	3.521066
228.232381	4161.507934	16.608128	-0.045982	3.517861
228.305443	4153.493299	16.613133	-0.045990	3.514651
228.460353	4145.514667	16.618138	-0.046014	3.511455
228.452606	4137.481163	16.623143	-0.046008	3.508230
228.368567	4129.471048	16.628147	-0.045987	3.505008
228.236578	4121.552739	16.633152	-0.045958	3.501819
228.265562	4113.541617	16.638157	-0.045958	3.498595
228.231616	4105.568328	16.643162	-0.045947	3.495380
228.085468	4097.570923	16.648167	-0.045915	3.492150
227.885862	4089.577445	16.653171	-0.045873	3.488917
228.006975	4081.591790	16.658176	-0.045890	3.485694
227.806026	4073.600229	16.663181	-0.045848	3.482455
227.659186	4065.621183	16.668186	-0.045816	3.479220
227.554483	4057.646298	16.673191	-0.045791	3.475985
227.756324	4049.575358	16.678195	-0.045824	3.472718
227.910179	4041.568770	16.683200	-0.045848	3.469472
227.646757	4033.604372	16.688205	-0.045794	3.466227
227.549887	4025.637331	16.693210	-0.045771	3.462983
227.624361	4017.645699	16.698215	-0.045780	3.459732
227.578346	4009.655134	16.703219	-0.045766	3.456474
227.487951	4001.642035	16.708224	-0.045744	3.453203
227.612457	3993.600150	16.713229	-0.045763	3.449923
227.506279	3985.657795	16.718234	-0.045738	3.446674
227.525739	3977.657886	16.723239	-0.045737	3.443402
227.524182	3969.682523	16.728243	-0.045731	3.440136
227.284843	3961.731041	16.733248	-0.045682	3.436869
227.332116	3953.681708	16.738253	-0.045686	3.433569
227.307821	3945.675585	16.743258	-0.045676	3.430280
227.128635	3937.716418	16.748263	-0.045638	3.427003
226.986560	3929.708055	16.753267	-0.045607	3.423703
227.002535	3921.745995	16.758272	-0.045605	3.420425
227.013042	3913.744326	16.763277	-0.045602	3.417127
226.935780	3905.744028	16.768282	-0.045582	3.413823
226.898848	3897.748172	16.773287	-0.045571	3.410519
226.841315	3889.747456	16.778291	-0.045555	3.407210
226.910614	3881.774895	16.783296	-0.045563	3.403913
226.763312	3873.815309	16.788301	-0.045531	3.400611
226.620024	3865.846634	16.793306	-0.045499	3.397302
226.730499	3857.816390	16.798311	-0.045515	3.393973
226.712064	3849.707922	16.803315	-0.045506	3.390604
226.667575	3841.768048	16.808320	-0.045493	3.387300
226.593437	3833.765734	16.813325	-0.045474	3.383966
226.722899	3825.790056	16.818330	-0.045494	3.380648
226.570834	3817.843795	16.823335	-0.045460	3.377328
226.353418	3809.841470	16.828339	-0.045415	3.373980
226.416278	3801.830028	16.833344	-0.045422	3.370634
226.223230	3793.856580	16.838349	-0.045381	3.367291
226.271691	3785.849602	16.843354	-0.045385	3.363940
226.368016	3777.872531	16.848359	-0.045398	3.360600
226.157661	3769.911133	16.853363	-0.045354	3.357252
226.105375	3761.930782	16.858368	-0.045339	3.353898
226.167703	3753.869124	16.863373	-0.045346	3.350511
226.266913	3745.876164	16.868378	-0.045359	3.347151
226.152784	3737.900070	16.873383	-0.045333	3.343787
225.821457	3729.935413	16.878387	-0.045267	3.340416
226.139152	3721.960084	16.883392	-0.045321	3.337061
225.933626	3713.943812	16.888397	-0.045278	3.333666
225.938509	3705.917387	16.893402	-0.045274	3.330271
225.793685	3697.960921	16.898407	-0.045242	3.326897
226.078576	3689.926959	16.903411	-0.045290	3.323502
225.967972	3682.006532	16.908416	-0.045264	3.320138
225.654777	3674.033469	16.913421	-0.045201	3.316740
225.620791	3666.019061	16.918426	-0.045190	3.313331
225.566187	3657.989821	16.923431	-0.045175	3.309912
225.515448	3650.001524	16.928435	-0.045160	3.306507
225.436776	3642.022508	16.933440	-0.045141	3.303101
225.200559	3634.054866	16.938445	-0.045092	3.299691
225.264468	3626.080404	16.943450	-0.045099	3.296285
225.167610	3618.072410	16.948455	-0.045076	3.292856
225.331505	3610.026787	16.953459	-0.045101	3.289416
225.191121	3602.104251	16.958464	-0.045070	3.286015
225.174879	3594.117708	16.963469	-0.045062	3.282587
225.431028	3586.084375	16.968474	-0.045105	3.279146
225.412742	3578.143002	16.973479	-0.045097	3.275730
225.116409	3570.135153	16.978483	-0.045037	3.272271
225.146924	3562.143093	16.983488	-0.045038	3.268828
225.027414	3554.132622	16.988493	-0.045010	3.265368
224.963123	3546.176233	16.993498	-0.044994	3.261929
224.926913	3538.183833	16.998503	-0.044982	3.258472
224.919891	3530.167694	17.003507	-0.044976	3.255003
224.833560	3522.191172	17.008512	-0.044955	3.251544
224.725961	3514.190609	17.013517	-0.044930	3.248069
224.577945	3506.203115	17.018522	-0.044897	3.244596
224.672954	3498.235494	17.023527	-0.044910	3.241136
224.673101	3490.252147	17.028531	-0.044905	3.237663
224.835385	3482.255134	17.033536	-0.044930	3.234186
224.581617	3474.204503	17.038541	-0.044878	3.230666
224.485779	3466.219513	17.043546	-0.044855	3.227176
224.416286	3458.245028	17.048551	-0.044837	3.223688
224.296217	3450.266833	17.053555	-0.044810	3.220193
224.388348	3442.298092	17.058560	-0.044822	3.216707
224.154315	3434.305303	17.063565	-0.044774	3.213194
224.129529	3426.297374	17.068570	-0.044764	3.209678
224.141304	3418.345200	17.073575	-0.044762	3.206184
224.094723	3410.344082	17.078579	-0.044748	3.202663
224.061303	3402.362586	17.083584	-0.044737	3.199147
223.896904	3394.400214	17.088589	-0.044701	3.195630
223.962916	3386.393629	17.093594	-0.044709	3.192099
223.969302	3378.371903	17.098599	-0.044705	3.188556
223.985561	3370.365910	17.103603	-0.044703	3.185015
224.153062	3362.435353	17.108608	-0.044729	3.181511
223.942287	3354.429422	17.113613	-0.044685	3.177953
223.841845	3346.464833	17.118618	-0.044662	3.174414
223.875734	3338.451977	17.123623	-0.044663	3.170856
223.708521	3330.440175	17.128627	-0.044627	3.167285
223.672118	3322.480185	17.133632	-0.044615	3.163739
223.692450	3314.485839	17.138637	-0.044614	3.160176
223.643381	3306.529620	17.143642	-0.044600	3.156623
223.501238	3298.518123	17.148647	-0.044569	3.153038
223.577568	3290.467982	17.153651	-0.044578	3.149440
223.431265	3282.544929	17.158656	-0.044546	3.145886
223.487663	3274.523351	17.163661	-0.044551	3.142292
223.402615	3266.569301	17.168666	-0.044531	3.138718
223.475467	3258.584519	17.173671	-0.044539	3.135134
223.239964	3250.585127	17.178675	-0.044490	3.131525
223.177442	3242.587694	17.183680	-0.044474	3.127920
223.073963	3234.600105	17.188685	-0.044450	3.124314
223.195435	3226.646492	17.193690	-0.044467	3.120729
223.039619	3218.701887	17.198695	-0.044434	3.117131
222.922685	3210.681293	17.203699	-0.044407	3.113497
223.236954	3202.659499	17.208704	-0.044460	3.109877
223.095116	3194.680762	17.213709	-0.044429	3.106252
222.884368	3186.704568	17.218714	-0.044385	3.102621
222.900267	3178.726755	17.223719	-0.044383	3.098995
222.855576	3170.732141	17.228723	-0.044370	3.095355
222.774022	3162.752722	17.233728	-0.044350	3.091715
222.581610	3154.769987	17.238733	-0.044309	3.088065
222.542914	3146.776473	17.243738	-0.044297	3.084412
222.621916	3138.816011	17.248743	-0.044307	3.080775
222.487847	3130.833370	17.253747	-0.044277	3.077115
222.606124	3122.819672	17.258752	-0.044294	3.073447
222.465521	3114.742586	17.263757	-0.044263	3.069733
222.389741	3106.782811	17.268762	-0.044244	3.066073
222.412050	3098.837478	17.273767	-0.044243	3.062419
222.343872	3090.853981	17.278771	-0.044225	3.058738
222.346527	3082.887745	17.283776	-0.044221	3.055065
222.205874	3074.892436	17.288781	-0.044190	3.051367
222.323855	3066.895778	17.293786	-0.044207	3.047676
222.280730	3058.932788	17.298791	-0.044194	3.043989
222.091364	3050.970350	17.303795	-0.044154	3.040290
222.197728	3042.991776	17.308800	-0.044168	3.036594
221.969515	3034.983025	17.313805	-0.044121	3.032863
221.916095	3026.982177	17.318810	-0.044106	3.029139
221.905885	3019.001436	17.323815	-0.044099	3.025422
221.835603	3011.012685	17.328819	-0.044081	3.021694
221.803220	3003.071976	17.333824	-0.044070	3.017986
221.763880	2995.060332	17.338829	-0.044058	3.014240
221.782511	2987.050586	17.343834	-0.044057	3.010492
221.758456	2979.080596	17.348839	-0.044047	3.006757
221.505647	2971.108037	17.353843	-0.043995	3.003004
221.702428	2963.142642	17.358848	-0.044027	2.999272
221.436895	2955.190153	17.363853	-0.043973	2.995519
221.431264	2947.165917	17.368858	-0.043967	2.991740
221.569305	2939.141875	17.373863	-0.043987	2.987964
221.657026	2931.115410	17.378867	-0.043999	2.984179
221.496580	2923.221214	17.383872	-0.043964	2.980439
221.448154	2915.230792	17.388877	-0.043950	2.976655
221.458353	2907.242317	17.393882	-0.043947	2.972870
221.237513	2899.267703	17.398887	-0.043901	2.969075
220.964639	2891.286655	17.403891	-0.043845	2.965269
221.092296	2883.317561	17.408896	-0.043864	2.961485
221.105548	2875.325051	17.413901	-0.043862	2.957679
221.090371	2867.333459	17.418906	-0.043854	2.953866
220.925818	2859.355262	17.423911	-0.043818	2.950048
220.943689	2851.345557	17.428915	-0.043817	2.946219
220.931971	2843.391167	17.433920	-0.043810	2.942409
220.901632	2835.405505	17.438925	-0.043799	2.938579
220.923605	2827.421330	17.443930	-0.043798	2.934748
220.886546	2819.439075	17.448935	-0.043787	2.930909
220.776349	2811.432501	17.453939	-0.043761	2.927050
220.960058	2803.459427	17.458944	-0.043790	2.923217
220.842401	2795.503224	17.463949	-0.043764	2.919371
220.642702	2787.551075	17.468954	-0.043722	2.915518
220.740907	2779.478784	17.473959	-0.043735	2.911617
220.569151	2771.484982	17.478963	-0.043698	2.907735
220.448220	2763.528493	17.483968	-0.043670	2.903868
220.500428	2755.566098	17.488973	-0.043675	2.900003
220.427259	2747.594181	17.493978	-0.043657	2.896121
220.344875	2739.619923	17.498983	-0.043637	2.892232
220.118894	2731.632091	17.503987	-0.043590	2.888324
220.131181	2723.645920	17.508992	-0.043587	2.884424
220.347079	2715.682927	17.513997	-0.043622	2.880541
219.998555	2707.736258	17.519002	-0.043552	2.876630
220.087611	2699.732543	17.524007	-0.043564	2.872710
220.123682	2691.717692	17.529011	-0.043566	2.868776
219.925107	2683.751575	17.534016	-0.043524	2.864847
219.800431	2675.809722	17.539021	-0.043496	2.860930
219.933488	2667.794739	17.544026	-0.043516	2.856985
219.901464	2659.848552	17.549031	-0.043505	2.853059
219.880619	2651.830035	17.554035	-0.043496	2.849093
219.690810	2643.889078	17.559040	-0.043456	2.845150
219.588385	2635.922266	17.564045	-0.043432	2.841194
219.469175	2627.930816	17.569050	-0.043405	2.837219
219.547852	2619.928735	17.574055	-0.043414	2.833244
219.532204	2611.914761	17.579059	-0.043406	2.829253
219.487308	2603.963616	17.584064	-0.043393	2.825285
219.292913	2596.008277	17.589069	-0.043352	2.821302
219.342515	2588.004506	17.594074	-0.043356	2.817302
219.389333	2580.032949	17.599079	-0.043360	2.813313
219.220865	2572.042679	17.604083	-0.043324	2.809296
219.188657	2564.081781	17.609088	-0.043313	2.805296
219.275511	2556.093708	17.614093	-0.043324	2.801284
219.353334	2548.126126	17.619098	-0.043334	2.797275
219.225412	2540.153527	17.624103	-0.043305	2.793247
219.044620	2532.159100	17.629107	-0.043267	2.789198
219.195792	2524.170519	17.634112	-0.043290	2.785166
219.048199	2516.226938	17.639117	-0.043257	2.781133
218.903359	2508.282339	17.644122	-0.043226	2.777094
218.784055	2500.310168	17.649127	-0.043198	2.773037
218.680656	2492.300045	17.654131	-0.043174	2.768955
218.744459	2484.318334	17.659136	-0.043181	2.764892
218.704562	2476.353756	17.664141	-0.043169	2.760825
218.645508	2468.398300	17.669146	-0.043153	2.756756
218.412166	2460.409908	17.674151	-0.043105	2.752653
218.307300	2452.369726	17.679155	-0.043080	2.748526
218.340146	2444.392875	17.684160	-0.043081	2.744433
218.444221	2436.432223	17.689165	-0.043096	2.740347
218.267093	2428.476094	17.694170	-0.043058	2.736239
218.468365	2420.462923	17.699175	-0.043090	2.732119
218.385889	2412.485167	17.704179	-0.043070	2.727994
218.322757	2404.541948	17.709184	-0.043053	2.723882
218.388575	2396.576116	17.714189	-0.043061	2.719760
218.296171	2388.627983	17.719194	-0.043039	2.715631
218.110224	2380.646737	17.724199	-0.042999	2.711472
218.082114	2372.645145	17.729203	-0.042989	2.707306
217.977953	2364.695532	17.734208	-0.042965	2.703157
217.958608	2356.712133	17.739213	-0.042956	2.698988
217.906497	2348.749196	17.744218	-0.042942	2.694822
217.884321	2340.781288	17.749223	-0.042933	2.690648
217.769375	2332.791746	17.754227	-0.042906	2.686451
217.725618	2324.851875	17.759232	-0.042893	2.682278
217.588156	2316.895409	17.764237	-0.042863	2.678084
217.614013	2308.894371	17.769242	-0.042863	2.673869
217.580161	2300.871806	17.774247	-0.042851	2.669633
217.561636	2292.901436	17.779251	-0.042843	2.665419
217.440645	2284.962061	17.784256	-0.042816	2.661208
217.193424	2277.017197	17.789261	-0.042765	2.656980
217.410327	2268.991362	17.794266	-0.042800	2.652731
217.550618	2261.013146	17.799271	-0.042821	2.648496
217.313329	2253.037425	17.804275	-0.042772	2.644231
217.171872	2245.121969	17.809280	-0.042741	2.639998
217.115969	2237.164407	17.814285	-0.042726	2.635741
217.120807	2229.143201	17.819290	-0.042722	2.631447
217.038599	2221.178691	17.824295	-0.042701	2.627170
216.927365	2213.213941	17.829299	-0.042676	2.622885
216.955700	2205.253393	17.834304	-0.042676	2.618604
216.865291	2197.281786	17.839309	-0.042654	2.614302
216.764448	2189.296908	17.844314	-0.042631	2.609985
216.897090	2181.340671	17.849319	-0.042650	2.605692
216.710205	2173.388030	17.854323	-0.042611	2.601372
216.685129	2165.432823	17.859328	-0.042601	2.597055
216.639963	2157.334356	17.864333	-0.042588	2.592651
216.571594	2149.263177	17.869338	-0.042570	2.588253
216.624702	2141.335833	17.874343	-0.042575	2.583935
216.503649	2133.406735	17.879347	-0.042548	2.579596
216.499945	2125.498239	17.884352	-0.042542	2.575269
216.343776	2117.519775	17.889357	-0.042508	2.570886
216.050582	2109.588199	17.894362	-0.042449	2.566512
216.406342	2101.590885	17.899367	-0.042510	2.562139
216.354137	2093.647013	17.904371	-0.042495	2.557760
216.369393	2085.695786	17.909376	-0.042493	2.553374
216.138796	2077.716888	17.914381	-0.042445	2.548947
216.177685	2069.720266	17.919386	-0.042448	2.544523
216.055352	2061.812597	17.924391	-0.042420	2.540128
216.107736	2053.822301	17.929395	-0.042425	2.535692
216.073206	2045.851161	17.934400	-0.042414	2.531253
216.122538	2037.850009	17.939405	-0.042418	2.526796
216.111575	2029.904446	17.944410	-0.042411	2.522357
215.981630	2022.008478	17.949415	-0.042382	2.517930
215.716665	2014.043368	17.954419	-0.042328	2.513446
215.662643	2006.027440	17.959424	-0.042313	2.508941
215.687745	1998.047625	17.964429	-0.042312	2.504454
215.555374	1990.110986	17.969434	-0.042283	2.499972
215.437182	1982.158093	17.974439	-0.042256	2.495473
215.383482	1974.162454	17.979443	-0.042241	2.490947
215.523416	1966.173617	17.984448	-0.042262	2.486431
215.413773	1958.255498	17.989453	-0.042237	2.481928
215.446016	1950.278791	17.994458	-0.042238	2.477394
215.428430	1942.332178	17.999463	-0.042230	2.472866
215.535522	1934.310371	18.004467	-0.042245	2.468295
215.406224	1926.386575	18.009472	-0.042216	2.463754
215.427387	1918.424301	18.014477	-0.042215	2.459194
215.561255	1910.439735	18.019482	-0.042235	2.454622
215.367933	1902.522084	18.024487	-0.042194	2.450054
215.089580	1894.549538	18.029491	-0.042137	2.445440
215.204073	1886.614028	18.034496	-0.042154	2.440869
215.218959	1878.641161	18.039501	-0.042151	2.436260
215.002194	1870.639900	18.044506	-0.042106	2.431607
214.928294	1862.652133	18.049511	-0.042088	2.426965
214.762396	1854.713578	18.054515	-0.042052	2.422335
214.682025	1846.785656	18.059520	-0.042032	2.417709
214.690612	1838.808792	18.064525	-0.042029	2.413053
214.639489	1830.832851	18.069530	-0.042014	2.408383
214.649801	1822.879393	18.074535	-0.042011	2.403723
214.584416	1814.943731	18.079539	-0.041994	2.399057
214.586417	1806.992281	18.084544	-0.041990	2.394379
214.724583	1798.977059	18.089549	-0.042010	2.389665
214.491287	1791.035717	18.094554	-0.041962	2.384955
214.559770	1783.116653	18.099559	-0.041970	2.380274
214.594715	1775.146618	18.104563	-0.041971	2.375550
214.428779	1767.196572	18.109568	-0.041936	2.370813
214.365552	1759.235594	18.114573	-0.041919	2.366067
214.374599	1751.284272	18.119578	-0.041916	2.361324
214.460037	1743.334164	18.124583	-0.041927	2.356579
214.154932	1735.370014	18.129587	-0.041865	2.351783
214.179771	1727.397896	18.134592	-0.041865	2.347000
214.039927	1719.463290	18.139597	-0.041834	2.342216
213.835700	1711.540004	18.144602	-0.041791	2.337424
213.798362	1703.585356	18.149607	-0.041779	2.332617
213.770806	1695.582920	18.154611	-0.041769	2.327771
213.754892	1687.652388	18.159616	-0.041761	2.322961
213.595460	1679.722725	18.164621	-0.041727	2.318128
213.653601	1671.734624	18.169626	-0.041733	2.313268
213.643416	1663.769034	18.174631	-0.041726	2.308406
213.636181	1655.806303	18.179635	-0.041719	2.303536
213.753268	1647.863182	18.184640	-0.041736	2.298678
213.558905	1639.936165	18.189645	-0.041695	2.293793
213.346420	1631.984565	18.194650	-0.041651	2.288881
213.285602	1624.046445	18.199655	-0.041635	2.283980
213.299166	1616.084852	18.204659	-0.041632	2.279060
213.264497	1608.145839	18.209664	-0.041621	2.274139
213.191007	1600.115617	18.214669	-0.041602	2.269147
213.099887	1592.167445	18.219674	-0.041580	2.264194
213.083750	1584.240808	18.224679	-0.041573	2.259250
212.820612	1576.307471	18.229683	-0.041519	2.254269
212.837523	1568.347618	18.234688	-0.041517	2.249286
212.810037	1560.399895	18.239693	-0.041507	2.244294
212.756886	1552.471952	18.244698	-0.041492	2.239302
212.747389	1544.534339	18.249703	-0.041485	2.234297
212.846807	1536.534612	18.254707	-0.041499	2.229250
212.649043	1528.621160	18.259712	-0.041457	2.224221
212.595060	1520.683933	18.264717	-0.041442	2.219178
212.576773	1512.735247	18.269722	-0.041434	2.214119
212.655093	1504.767654	18.274727	-0.041444	2.209045
212.386088	1496.841392	18.279731	-0.041389	2.203954
212.523801	1488.910772	18.284736	-0.041410	2.198886
212.355085	1480.976799	18.289741	-0.041373	2.193776
212.394200	1472.982585	18.294746	-0.041376	2.188634
212.129449	1465.068782	18.299751	-0.041321	2.183505
212.093781	1457.123399	18.304755	-0.041310	2.178363
212.138700	1449.177634	18.309760	-0.041313	2.173217
212.098393	1441.225333	18.314765	-0.041301	2.168046
212.031346	1433.285530	18.319770	-0.041284	2.162869
212.094591	1425.366001	18.324775	-0.041290	2.157705
211.937058	1417.417814	18.329779	-0.041256	2.152488
211.917589	1409.470190	18.334784	-0.041248	2.147273
211.959530	1401.537104	18.339789	-0.041251	2.142060
211.910536	1393.604159	18.344794	-0.041237	2.136826
211.827539	1385.677857	18.349799	-0.041216	2.131580
211.608301	1377.739636	18.354803	-0.041171	2.126300
211.691520	1369.794383	18.359808	-0.041181	2.121031
211.576402	1361.883809	18.364813	-0.041155	2.115754
211.536552	1353.868186	18.369818	-0.041142	2.110400
211.370717	1345.949372	18.374823	-0.041107	2.105085
211.338380	1338.017853	18.379827	-0.041096	2.099761
211.331153	1330.097945	18.384832	-0.041090	2.094434
211.313065	1322.152349	18.389837	-0.041081	2.089074
211.108560	1314.233706	18.394842	-0.041038	2.083701
211.100609	1306.318514	18.399847	-0.041032	2.078336
211.190972	1298.360548	18.404851	-0.041044	2.072937
211.172306	1290.422886	18.409856	-0.041036	2.067528
210.977902	1282.522768	18.414861	-0.040995	2.062112
210.901273	1274.596023	18.419866	-0.040975	2.056675
211.000897	1266.656958	18.424871	-0.040989	2.051234
211.004335	1258.699085	18.429875	-0.040985	2.045755
210.757381	1250.820055	18.434880	-0.040934	2.040290
210.787245	1242.886680	18.439885	-0.040935	2.034802
210.576163	1234.945915	18.444890	-0.040890	2.029269
210.714428	1226.992454	18.449895	-0.040911	2.023747
210.622867	1219.072833	18.454899	-0.040889	2.018211
210.545423	1211.169561	18.459904	-0.040870	2.012672
210.542346	1203.223982	18.464909	-0.040865	2.007095
210.313722	1195.325031	18.469914	-0.040817	2.001513
210.450761	1187.399964	18.474919	-0.040838	1.995935
210.190204	1179.478028	18.479923	-0.040784	1.990301
210.353662	1171.527247	18.484928	-0.040810	1.984676
210.276437	1163.636022	18.489933	-0.040791	1.979052
210.268296	1155.700393	18.494938	-0.040784	1.973387
209.969529	1147.811776	18.499943	-0.040724	1.967709
209.925244	1139.892013	18.504947	-0.040711	1.962019
210.027019	1131.978336	18.509952	-0.040725	1.956332
209.911302	1124.029287	18.514957	-0.040698	1.950580
209.834706	1116.078074	18.519962	-0.040679	1.944814
209.981545	1108.167529	18.524967	-0.040702	1.939084
209.948686	1100.242860	18.529971	-0.040691	1.933307
209.776020	1092.344383	18.534976	-0.040654	1.927517
209.604931	1084.444632	18.539981	-0.040617	1.921709
209.692714	1076.524034	18.544986	-0.040628	1.915896
209.554123	1068.632020	18.549991	-0.040598	1.910061
209.328185	1060.729179	18.554995	-0.040551	1.904191
209.219596	1052.835585	18.560000	-0.040526	1.898323
209.343128	1044.896024	18.565005	-0.040544	1.892428
209.208917	1036.976199	18.570010	-0.040514	1.886500
209.353103	1029.067680	18.575015	-0.040536	1.880594
209.208652	1021.184276	18.580019	-0.040504	1.874655
208.985221	1013.283608	18.585024	-0.040458	1.868676
209.098494	1005.344770	18.590029	-0.040474	1.862686
208.972813	997.454328	18.595034	-0.040446	1.856687
209.139206	989.522187	18.600039	-0.040472	1.850670
208.731926	981.659558	18.605043	-0.040391	1.844620
208.812882	973.762303	18.610048	-0.040401	1.838581
208.809646	965.850902	18.615053	-0.040396	1.832501
208.781513	957.938427	18.620058	-0.040386	1.826397
208.651301	950.062483	18.625063	-0.040356	1.820288
208.611821	942.169535	18.630067	-0.040344	1.814157
208.554717	934.270774	18.635072	-0.040329	1.807998
208.296129	926.407180	18.640077	-0.040276	1.801821
208.167622	918.527144	18.645082	-0.040247	1.795626
208.224085	910.569251	18.650087	-0.040253	1.789370
208.034912	902.674867	18.655091	-0.040213	1.783113
208.049508	894.785093	18.660096	-0.040210	1.776862
208.015585	886.883747	18.665101	-0.040199	1.770574
208.019678	878.993203	18.670106	-0.040195	1.764277
208.214216	871.099695	18.675111	-0.040226	1.757979
207.984783	863.229739	18.680115	-0.040179	1.751623
207.980766	855.339728	18.685120	-0.040173	1.745257
207.861960	847.487200	18.690125	-0.040146	1.738884
207.731804	839.617760	18.695130	-0.040117	1.732471
207.727405	831.724356	18.700135	-0.040112	1.726032
207.542784	823.869663	18.705139	-0.040072	1.719577
207.301801	816.028627	18.710144	-0.040023	1.713101
207.461540	808.085154	18.715149	-0.040048	1.706568
207.371211	800.213972	18.720154	-0.040026	1.700038
207.290216	792.370842	18.725159	-0.040006	1.693506
207.325155	784.454721	18.730163	-0.040008	1.686904
207.320664	776.587640	18.735168	-0.040002	1.680312
207.143951	768.756270	18.740173	-0.039964	1.673701
207.127177	760.861767	18.745178	-0.039956	1.667031
207.250664	752.987545	18.750183	-0.039974	1.660371
206.883783	745.177002	18.755187	-0.039901	1.653672
206.933069	737.293674	18.760192	-0.039906	1.646940
206.843719	729.446241	18.765197	-0.039884	1.640193
206.871543	721.564340	18.770202	-0.039884	1.633403
206.752694	713.668007	18.775207	-0.039857	1.626553
206.706860	705.812663	18.780211	-0.039844	1.619719
206.822183	697.946778	18.785216	-0.039861	1.612870
206.534593	690.128462	18.790221	-0.039802	1.605977
206.414898	682.293979	18.795226	-0.039775	1.599063
206.499158	674.448302	18.800231	-0.039786	1.592138
206.349466	666.591645	18.805235	-0.039753	1.585140
206.228252	658.771990	18.810240	-0.039726	1.578148
206.263035	650.911627	18.815245	-0.039728	1.571111
206.145054	643.074358	18.820250	-0.039701	1.564041
206.125453	635.257695	18.825255	-0.039692	1.556971
205.962268	627.416212	18.830259	-0.039657	1.549826
205.910851	619.576652	18.835264	-0.039643	1.542666
205.936697	611.736113	18.840269	-0.039643	1.535483
205.917196	603.894874	18.845274	-0.039634	1.528259
205.798047	596.091711	18.850279	-0.039607	1.521021
205.589735	588.298892	18.855283	-0.039564	1.513744
205.658623	580.443816	18.860288	-0.039572	1.506416
205.569828	572.643409	18.865293	-0.039550	1.499079
205.535832	564.811665	18.870298	-0.039539	1.491686
205.404856	557.019292	18.875303	-0.039510	1.484277
205.266183	549.225472	18.880307	-0.039479	1.476829
205.159595	541.377657	18.885312	-0.039455	1.469296
205.191622	533.544923	18.890317	-0.039456	1.461761
204.964920	525.774211	18.895322	-0.039409	1.454206
205.043570	517.952179	18.900327	-0.039419	1.446610
204.741842	510.198356	18.905331	-0.039358	1.438980
204.704507	502.403667	18.910336	-0.039346	1.431311
204.927573	494.567037	18.915341	-0.039383	1.423602
204.696509	486.811199	18.920346	-0.039335	1.415857
204.552923	479.040184	18.925351	-0.039303	1.408069
204.737990	471.217945	18.930355	-0.039333	1.400240
204.785308	463.440218	18.935360	-0.039337	1.392389
204.361279	455.711236	18.940365	-0.039253	1.384464
204.284470	447.940721	18.945370	-0.039234	1.376510
204.181772	440.179125	18.950375	-0.039210	1.368514
204.043964	432.418770	18.955379	-0.039180	1.360466
203.910220	424.679911	18.960384	-0.039150	1.352394
203.991824	416.897041	18.965389	-0.039161	1.344264
203.873077	409.154805	18.970394	-0.039134	1.336093
203.904712	401.396722	18.975399	-0.039135	1.327881
203.484827	393.703633	18.980403	-0.039052	1.319606
203.465973	385.890904	18.985408	-0.039044	1.311223
203.460518	378.089570	18.990413	-0.039038	1.302801
203.342415	370.373077	18.995418	-0.039011	1.294396
203.413757	362.632632	19.000423	-0.039020	1.285944
203.150126	354.963917	19.005427	-0.038966	1.277454
203.170053	347.238544	19.010432	-0.038965	1.268896
203.348695	339.500757	19.015437	-0.038993	1.260297
203.079743	331.832572	19.020442	-0.038938	1.251632
203.027407	324.143227	19.025447	-0.038924	1.242924
202.882124	316.471453	19.030451	-0.038892	1.234156
202.858163	308.759350	19.035456	-0.038883	1.225303
202.585673	301.121405	19.040461	-0.038828	1.216422
202.341886	293.460173	19.045466	-0.038778	1.207455
202.328447	285.792032	19.050471	-0.038770	1.198458
202.284359	278.118920	19.055475	-0.038757	1.189382
202.269275	270.456709	19.060480	-0.038750	1.180254
202.108234	262.825881	19.065485	-0.038715	1.171063
201.913317	255.199342	19.070490	-0.038674	1.161797
201.959529	247.546819	19.075495	-0.038678	1.152476
201.575007	239.933550	19.080499	-0.038602	1.143036
201.798491	232.265647	19.085504	-0.038639	1.133579
201.649191	224.663812	19.090509	-0.038606	1.124045
201.330229	217.107228	19.095514	-0.038542	1.114449
201.302959	209.505761	19.100519	-0.038532	1.104777
201.164035	201.933328	19.105523	-0.038502	1.095032
200.946940	194.374440	19.110528	-0.038457	1.085200
200.868095	186.814966	19.115533	-0.038438	1.075308
200.698640	179.249134	19.120538	-0.038401	1.065295
200.457093	171.734206	19.125543	-0.038352	1.055239
200.217334	164.205876	19.130547	-0.038302	1.045067
200.097618	156.695689	19.135552	-0.038276	1.034849
199.816005	149.205580	19.140557	-0.038219	1.024518
199.318912	141.763524	19.145562	-0.038121	1.014096
199.042403	134.297322	19.150567	-0.038065	1.003586
198.868182	126.809486	19.155571	-0.038028	0.992959
198.505241	119.355370	19.160576	-0.037956	0.982218
197.755117	111.997705	19.165581	-0.037812	0.971400
196.713164	104.690585	19.170586	-0.037613	0.960459
195.624030	97.401721	19.175591	-0.037406	0.949406
194.198112	90.162589	19.180595	-0.037136	0.938209
193.152956	82.864981	19.185600	-0.036937	0.926888
192.200326	75.576475	19.190605	-0.036755	0.915466
191.078825	68.294774	19.195610	-0.036542	0.903863
190.404276	61.201434	19.200615	-0.036412	0.892531