Thu Mar 11 18:40:19 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.222975	-0.161844	0.000000	-0.000058	0.724895

0.340098	-0.185985	0.005005	-0.000080	0.724889
0.388122	-0.194114	0.010010	-0.000090	0.724891
0.369521	-0.195728	0.015014	-0.000086	0.724881
0.585160	-0.228510	0.020019	-0.000127	0.724893
0.278956	-0.177327	0.025024	-0.000070	0.724887
0.153662	-0.154521	0.030029	-0.000047	0.724888
0.280158	-0.175304	0.035034	-0.000071	0.724892
0.254872	-0.174690	0.040038	-0.000067	0.724885
0.215984	-0.164354	0.045043	-0.000060	0.724892
0.340141	-0.188471	0.050048	-0.000083	0.724889
0.357760	-0.192064	0.055053	-0.000086	0.724888
0.209144	-0.181902	0.060058	-0.000059	0.724857
0.239126	-0.325189	0.065062	-0.000065	0.724588
0.209866	-0.314814	0.070067	-0.000060	0.724598
0.129361	-0.303251	0.075072	-0.000045	0.724593
0.178834	-0.312596	0.080077	-0.000054	0.724593
0.302956	-0.331521	0.085082	-0.000078	0.724600
0.130174	-0.306881	0.090086	-0.000046	0.724588
0.142207	-0.386400	0.095091	-0.000048	0.724437
0.047604	-0.462067	0.100096	-0.000031	0.724257
0.156802	-0.479692	0.105101	-0.000052	0.724261
0.214707	-0.487907	0.110106	-0.000063	0.724265
0.221391	-0.492464	0.115110	-0.000064	0.724259
0.287346	-0.560665	0.120115	-0.000077	0.724149
0.391340	-0.680378	0.125120	-0.000096	0.723951
0.047738	-0.619940	0.130125	-0.000032	0.723950
0.195957	-0.642841	0.135130	-0.000060	0.723958
0.145012	-0.661759	0.140134	-0.000051	0.723903
0.243039	-0.814749	0.145139	-0.000070	0.723638
0.172262	-0.808220	0.150144	-0.000057	0.723627
0.207064	-0.812962	0.155149	-0.000063	0.723630
-0.053415	-0.823553	0.160154	-0.000015	0.723519
-0.049059	-0.918949	0.165158	-0.000016	0.723334
0.114034	-0.941875	0.170163	-0.000047	0.723347
0.134771	-0.950283	0.175168	-0.000051	0.723338
0.074370	-1.096808	0.180173	-0.000040	0.723030
0.173393	-1.125680	0.185178	-0.000059	0.723009
0.103148	-1.117887	0.190182	-0.000046	0.723000
0.213819	-1.260788	0.195187	-0.000067	0.722759
0.275589	-1.307486	0.200192	-0.000078	0.722689
0.298686	-1.311140	0.205197	-0.000083	0.722690
0.076153	-1.431319	0.210202	-0.000042	0.722377
0.071926	-1.436867	0.215206	-0.000041	0.722365
0.104347	-1.474305	0.220211	-0.000047	0.722304
0.055026	-1.585659	0.225216	-0.000038	0.722068
-0.131713	-1.550878	0.230221	-0.000004	0.722072
-0.101781	-1.651752	0.235226	-0.000010	0.721885
0.090130	-1.758843	0.240230	-0.000046	0.721742
0.060013	-1.768316	0.245235	-0.000040	0.721713
-0.187891	-1.863866	0.250240	0.000006	0.721439
-0.260120	-1.851421	0.255245	0.000019	0.721439
-0.141748	-1.979114	0.260250	-0.000003	0.721230
-0.017779	-2.058842	0.265254	-0.000027	0.721117
-0.049834	-2.096689	0.270259	-0.000021	0.721032
-0.078946	-2.170646	0.275264	-0.000016	0.720877
-0.414059	-2.137810	0.280269	0.000046	0.720824
-0.809864	-2.206726	0.285274	0.000120	0.720551
-3.592534	-1.719655	0.290278	0.000637	0.720534
-2.863902	-1.882619	0.295283	0.000502	0.720470
-4.029798	-1.802465	0.300288	0.000718	0.720219
-4.502606	-1.718087	0.305293	0.000806	0.720220
-4.288862	-1.752010	0.310298	0.000766	0.720229
-4.166963	-1.783250	0.315302	0.000743	0.720210
-4.977641	-1.795937	0.320307	0.000894	0.719902
-5.549319	-1.697238	0.325312	0.001000	0.719896
-5.563020	-1.692838	0.330317	0.001002	0.719900
-5.000213	-1.792176	0.335322	0.000897	0.719903
-5.610199	-1.694419	0.340326	0.001010	0.719882
-5.989905	-1.768098	0.345331	0.001081	0.719604
-5.838281	-1.798408	0.350336	0.001052	0.719598
-6.315091	-1.712838	0.355341	0.001141	0.719600
-6.027010	-1.762659	0.360346	0.001087	0.719603
-6.114290	-1.752124	0.365350	0.001103	0.719594
-6.730314	-1.793235	0.370355	0.001217	0.719297
-6.954684	-1.768297	0.375360	0.001259	0.719268
-6.850488	-1.787508	0.380365	0.001239	0.719267
-6.693015	-1.811971	0.385370	0.001210	0.719274
-7.409211	-1.688635	0.390374	0.001343	0.719267
-6.858506	-1.848355	0.395379	0.001240	0.719146
-7.806737	-1.774737	0.400384	0.001416	0.718958
-8.030828	-1.734174	0.405389	0.001458	0.718960
-8.234037	-1.694245	0.410394	0.001495	0.718968
-7.988955	-1.742662	0.415398	0.001449	0.718959
-8.117647	-1.715766	0.420403	0.001473	0.718967
-8.360064	-1.699355	0.425408	0.001518	0.718915
-9.102177	-1.706070	0.430413	0.001656	0.718641
-8.658708	-1.782503	0.435418	0.001573	0.718647
-9.393439	-1.654671	0.440422	0.001709	0.718642
-9.212128	-1.683227	0.445427	0.001675	0.718649
-8.824886	-1.756131	0.450432	0.001603	0.718642
-8.984050	-1.728318	0.455437	0.001632	0.718642
-8.797184	-1.815831	0.460442	0.001597	0.718535
-9.899925	-1.713574	0.465446	0.001802	0.718350
-9.590172	-1.764139	0.470451	0.001745	0.718359
-9.813759	-1.728132	0.475456	0.001786	0.718352
-9.777121	-1.733531	0.480461	0.001779	0.718355
-9.689388	-1.747715	0.485466	0.001762	0.718358
-10.393186	-1.627997	0.490470	0.001893	0.718348
-10.047998	-1.813631	0.495475	0.001828	0.718103
-10.535777	-1.771617	0.500480	0.001919	0.718015
-11.047547	-1.683093	0.505485	0.002014	0.718010
-10.885833	-1.706622	0.510490	0.001984	0.718021
-10.915987	-1.706606	0.515494	0.001989	0.718011
-10.610512	-1.757875	0.520499	0.001932	0.718018
-10.902283	-1.706915	0.525504	0.001986	0.718016
-11.441773	-1.745818	0.530509	0.002086	0.717750
-11.564234	-1.746655	0.535514	0.002109	0.717706
-11.707454	-1.724838	0.540518	0.002135	0.717699
-11.886216	-1.690807	0.545523	0.002168	0.717704
-11.909325	-1.688015	0.550528	0.002172	0.717702
-12.057750	-1.663218	0.555533	0.002199	0.717699
-11.592776	-1.743452	0.560538	0.002113	0.717705
-11.688892	-1.806667	0.565542	0.002130	0.717546
-12.725617	-1.704966	0.570547	0.002323	0.717383
-12.567766	-1.736380	0.575552	0.002293	0.717377
-12.886287	-1.679626	0.580557	0.002352	0.717377
-12.629114	-1.722573	0.585562	0.002304	0.717384
-13.118726	-1.640792	0.590566	0.002395	0.717373
-13.056707	-1.646413	0.595571	0.002383	0.717385
-12.532147	-1.751236	0.600576	0.002285	0.717363
-13.245120	-1.766483	0.605581	0.002418	0.717082
-13.781090	-1.668786	0.610586	0.002517	0.717087
-13.828452	-1.664237	0.615590	0.002526	0.717080
-13.167740	-1.780013	0.620595	0.002403	0.717084
-13.579323	-1.706801	0.625600	0.002479	0.717084
-14.172804	-1.602647	0.630605	0.002589	0.717082
-13.317027	-1.750999	0.635610	0.002430	0.717090
-14.089417	-1.750397	0.640614	0.002573	0.716820
-15.075457	-1.604316	0.645619	0.002756	0.716762
-14.635749	-1.686013	0.650624	0.002674	0.716755
-14.523617	-1.709044	0.655629	0.002653	0.716750
-14.719167	-1.670960	0.660634	0.002689	0.716757
-14.633368	-1.688314	0.665638	0.002673	0.716753
-14.538802	-1.704195	0.670643	0.002655	0.716756
-14.859825	-1.659415	0.675648	0.002715	0.716732
-15.426757	-1.703257	0.680653	0.002820	0.716445
-15.231224	-1.735310	0.685658	0.002783	0.716451
-15.809822	-1.638375	0.690662	0.002891	0.716440
-15.481747	-1.691712	0.695667	0.002829	0.716450
-15.343518	-1.718682	0.700672	0.002803	0.716446
-15.262105	-1.733836	0.705677	0.002788	0.716446
-15.616937	-1.667734	0.710682	0.002854	0.716452
-16.168611	-1.701388	0.715686	0.002956	0.716191
-16.011740	-1.755989	0.720691	0.002927	0.716139
-16.142406	-1.736753	0.725696	0.002951	0.716131
-16.675286	-1.642361	0.730701	0.003050	0.716131
-16.502055	-1.671271	0.735706	0.003017	0.716135
-16.411295	-1.690770	0.740710	0.003000	0.716129
-16.699076	-1.636612	0.745715	0.003053	0.716135
-16.575619	-1.713307	0.750720	0.003030	0.716027
-17.222716	-1.673524	0.755725	0.003150	0.715878
-16.829294	-1.740006	0.760730	0.003077	0.715886
-17.101641	-1.695371	0.765734	0.003127	0.715879
-16.935050	-1.721013	0.770739	0.003096	0.715887
-17.044219	-1.705722	0.775744	0.003116	0.715879
-17.281033	-1.663361	0.780749	0.003160	0.715880
-17.044514	-1.847705	0.785754	0.003116	0.715599
-18.030339	-1.702107	0.790758	0.003299	0.715540
-18.315856	-1.648234	0.795763	0.003352	0.715546
-17.760486	-1.748727	0.800768	0.003248	0.715544
-17.974758	-1.712270	0.805773	0.003288	0.715541
-18.017690	-1.700077	0.810778	0.003295	0.715551
-18.112483	-1.711711	0.815782	0.003313	0.715494
-18.806116	-1.720240	0.820787	0.003442	0.715233
-18.737981	-1.735075	0.825792	0.003429	0.715228
-19.554826	-1.591349	0.830797	0.003580	0.715225
-18.881875	-1.706651	0.835802	0.003455	0.715235
-18.741296	-1.737028	0.840806	0.003428	0.715225
-19.034350	-1.679925	0.845811	0.003483	0.715235
-18.892119	-1.708786	0.850816	0.003456	0.715228
-19.451076	-1.767094	0.855821	0.003560	0.714916
-19.877854	-1.692579	0.860826	0.003639	0.714913
-20.152534	-1.648583	0.865830	0.003690	0.714904
-19.781064	-1.711164	0.870835	0.003620	0.714912
-19.829382	-1.705724	0.875840	0.003629	0.714906
-20.298312	-1.622442	0.880845	0.003716	0.714906
-19.618095	-1.741167	0.885850	0.003589	0.714911
-19.909945	-1.792340	0.890854	0.003643	0.714707
-21.162904	-1.618795	0.895859	0.003876	0.714609
-20.802640	-1.685476	0.900864	0.003809	0.714604
-20.792887	-1.688179	0.905869	0.003807	0.714603
-20.885623	-1.667395	0.910874	0.003824	0.714612
-21.013570	-1.650204	0.915878	0.003847	0.714601
-20.788195	-1.686565	0.920883	0.003805	0.714609
-20.656359	-1.768722	0.925888	0.003781	0.714493
-22.151960	-1.612050	0.930893	0.004059	0.714276
-21.707193	-1.688993	0.935898	0.003976	0.714281
-21.915991	-1.657828	0.940902	0.004014	0.714269
-21.714963	-1.687221	0.945907	0.003976	0.714283
-21.900065	-1.658548	0.950912	0.004011	0.714275
-21.974596	-1.646471	0.955917	0.004024	0.714273
-21.561349	-1.716541	0.960922	0.003947	0.714280
-22.326301	-1.709015	0.965926	0.004089	0.714025
-22.921817	-1.630746	0.970931	0.004200	0.713970
-22.623645	-1.685541	0.975936	0.004144	0.713967
-22.846063	-1.646722	0.980941	0.004185	0.713966
-22.870793	-1.638607	0.985946	0.004190	0.713974
-22.893628	-1.639195	0.990950	0.004194	0.713965
-22.703473	-1.670150	0.995955	0.004158	0.713972
-23.266524	-1.572057	1.000960	0.004262	0.713968
-23.382332	-1.706974	1.005965	0.004284	0.713659
-23.407984	-1.704781	1.010970	0.004288	0.713655
-24.436455	-1.526079	1.015974	0.004479	0.713646
-23.602177	-1.670384	1.020979	0.004324	0.713656
-23.398113	-1.709394	1.025984	0.004286	0.713651
-23.999928	-1.603292	1.030989	0.004397	0.713649
-23.565423	-1.676999	1.035994	0.004316	0.713657
-23.558067	-1.749810	1.040998	0.004315	0.713515
-24.565388	-1.649042	1.046003	0.004502	0.713359
-24.499773	-1.659656	1.051008	0.004489	0.713362
-24.755875	-1.617384	1.056013	0.004537	0.713356
-24.422977	-1.673070	1.061018	0.004475	0.713364
-24.486463	-1.667942	1.066022	0.004486	0.713352
-24.521097	-1.658379	1.071027	0.004492	0.713359
-24.449111	-1.754718	1.076032	0.004479	0.713193
-25.795502	-1.602123	1.081037	0.004729	0.713020
-25.120115	-1.718953	1.086042	0.004603	0.713028
-25.482341	-1.661339	1.091046	0.004670	0.713014
-25.660658	-1.626138	1.096051	0.004703	0.713022
-25.581377	-1.642247	1.101056	0.004688	0.713018
-25.418627	-1.672092	1.106061	0.004657	0.713017
-25.530294	-1.689513	1.111066	0.004678	0.712943
-26.949029	-1.556529	1.116070	0.004942	0.712705
-26.880951	-1.567075	1.121075	0.004929	0.712709
-26.445337	-1.645969	1.126080	0.004848	0.712707
-26.583151	-1.623866	1.131085	0.004873	0.712703
-26.699785	-1.598795	1.136090	0.004894	0.712712
-26.631021	-1.615343	1.141094	0.004881	0.712704
-26.267740	-1.676762	1.146099	0.004813	0.712711
-26.460203	-1.677458	1.151104	0.004849	0.712642
-27.672282	-1.593110	1.156109	0.005074	0.712380
-26.917249	-1.723945	1.161114	0.004934	0.712388
-27.608921	-1.604093	1.166118	0.005062	0.712382
-27.489876	-1.622389	1.171123	0.005040	0.712388
-27.016936	-1.707739	1.176128	0.004951	0.712386
-27.567962	-1.613066	1.181133	0.005054	0.712380
-27.704586	-1.584121	1.186138	0.005079	0.712390
-27.798983	-1.686536	1.191142	0.005096	0.712153
-28.358652	-1.619656	1.196147	0.005200	0.712088
-28.348799	-1.622100	1.201152	0.005198	0.712087
-28.153964	-1.658015	1.206157	0.005161	0.712085
-27.881261	-1.702165	1.211162	0.005110	0.712094
-28.296741	-1.633520	1.216166	0.005187	0.712084
-28.477301	-1.598276	1.221171	0.005221	0.712091
-28.536714	-1.701586	1.226176	0.005232	0.711864
-29.501442	-1.585218	1.231181	0.005411	0.711754
-29.330706	-1.612611	1.236186	0.005379	0.711760
-29.158757	-1.648794	1.241190	0.005347	0.711750
-28.998804	-1.674579	1.246195	0.005317	0.711756
-29.254241	-1.629437	1.251200	0.005364	0.711756
-29.647507	-1.560402	1.256205	0.005437	0.711754
-29.176202	-1.674470	1.261210	0.005349	0.711695
-30.031924	-1.646383	1.266214	0.005508	0.711447
-30.001469	-1.648898	1.271219	0.005502	0.711453
-30.183499	-1.616680	1.276224	0.005536	0.711453
-30.249664	-1.609451	1.281229	0.005548	0.711445
-29.885558	-1.669700	1.286234	0.005480	0.711455
-30.288947	-1.602263	1.291238	0.005554	0.711446
-30.164325	-1.630010	1.296243	0.005531	0.711436
-30.667214	-1.690208	1.301248	0.005624	0.711137
-31.152951	-1.606607	1.306253	0.005714	0.711132
-30.931068	-1.642688	1.311258	0.005673	0.711139
-30.845759	-1.662489	1.316262	0.005657	0.711131
-31.419195	-1.555634	1.321267	0.005763	0.711141
-30.984381	-1.633140	1.326272	0.005682	0.711141
-30.908793	-1.649449	1.331277	0.005668	0.711136
-31.370071	-1.675514	1.336282	0.005753	0.710920
-32.107577	-1.573356	1.341286	0.005890	0.710862
-31.674698	-1.646375	1.346291	0.005809	0.710871
-31.383533	-1.699301	1.351296	0.005755	0.710870
-32.239838	-1.548723	1.356301	0.005914	0.710866
-31.746326	-1.632078	1.361306	0.005822	0.710876
-31.622116	-1.660217	1.366310	0.005799	0.710864
-32.440601	-1.674948	1.371315	0.005951	0.710544
-32.840620	-1.609351	1.376320	0.006025	0.710533
-32.974134	-1.587457	1.381325	0.006049	0.710530
-32.793440	-1.616634	1.386330	0.006016	0.710536
-33.063740	-1.572747	1.391334	0.006066	0.710528
-32.633284	-1.646745	1.396339	0.005985	0.710534
-32.699448	-1.634509	1.401344	0.005997	0.710536
-33.015121	-1.682321	1.406349	0.006056	0.710328
-33.853479	-1.588056	1.411354	0.006212	0.710219
-33.642616	-1.628704	1.416358	0.006172	0.710213
-33.698586	-1.615316	1.421363	0.006182	0.710220
-33.673547	-1.620856	1.426368	0.006177	0.710219
-33.470062	-1.661634	1.431373	0.006139	0.710210
-33.715994	-1.612401	1.436378	0.006185	0.710222
-34.121485	-1.620650	1.441382	0.006260	0.710061
-34.664225	-1.607660	1.446387	0.006361	0.709894
-34.141731	-1.702439	1.451392	0.006263	0.709892
-34.606940	-1.618267	1.456397	0.006349	0.709895
-34.758266	-1.590815	1.461402	0.006377	0.709896
-34.351511	-1.666334	1.466406	0.006301	0.709891
-34.552947	-1.628468	1.471411	0.006339	0.709895
-34.805801	-1.644052	1.476416	0.006385	0.709774
-35.708659	-1.575352	1.481421	0.006553	0.709590
-35.323208	-1.639231	1.486426	0.006481	0.709601
-35.519224	-1.608067	1.491430	0.006517	0.709593
-35.494434	-1.612548	1.496435	0.006513	0.709594
-35.389672	-1.631516	1.501440	0.006493	0.709594
-35.936839	-1.536444	1.506445	0.006594	0.709589
-35.685371	-1.576523	1.511450	0.006547	0.709599
-35.886000	-1.704019	1.516454	0.006584	0.709273
-36.579234	-1.585018	1.521459	0.006713	0.709265
-36.739930	-1.556090	1.526464	0.006743	0.709266
-36.269272	-1.643428	1.531469	0.006655	0.709259
-36.414050	-1.614334	1.536474	0.006682	0.709267
-36.795878	-1.550598	1.541478	0.006752	0.709258
-36.527326	-1.595091	1.546483	0.006702	0.709266
-36.301662	-1.712355	1.551488	0.006660	0.709112
-37.653643	-1.552169	1.556493	0.006911	0.708951
-37.167277	-1.634509	1.561498	0.006821	0.708960
-37.331857	-1.610347	1.566502	0.006851	0.708950
-37.423905	-1.590730	1.571507	0.006868	0.708957
-37.499496	-1.578490	1.576512	0.006882	0.708955
-37.098908	-1.651235	1.581517	0.006807	0.708953
-36.979421	-1.751022	1.586522	0.006784	0.708796
-38.142619	-1.625727	1.591526	0.007001	0.708633
-37.955347	-1.656400	1.596531	0.006965	0.708639
-38.001443	-1.649768	1.601536	0.006974	0.708636
-38.494775	-1.565996	1.606541	0.007065	0.708628
-38.109913	-1.629977	1.611546	0.006993	0.708638
-38.011814	-1.650368	1.616550	0.006975	0.708633
-38.399773	-1.683557	1.621555	0.007047	0.708428
-39.160658	-1.588866	1.626560	0.007188	0.708347
-38.969611	-1.625745	1.631565	0.007152	0.708341
-38.577776	-1.691128	1.636570	0.007079	0.708351
-39.366871	-1.556586	1.641574	0.007226	0.708339
-39.203609	-1.582086	1.646579	0.007195	0.708347
-38.662969	-1.679522	1.651584	0.007094	0.708345
-39.149972	-1.726473	1.656589	0.007185	0.708078
-39.907289	-1.622896	1.661594	0.007325	0.708015
-39.955184	-1.619405	1.666598	0.007334	0.708006
-39.677106	-1.667670	1.671603	0.007282	0.708009
-39.832892	-1.639149	1.676608	0.007311	0.708011
-40.050449	-1.605496	1.681613	0.007351	0.708001
-39.673233	-1.668822	1.686618	0.007280	0.708009
-40.416972	-1.686172	1.691622	0.007419	0.707709
-40.946957	-1.599241	1.696627	0.007517	0.707695
-40.657635	-1.650601	1.701632	0.007463	0.707696
-40.855984	-1.616556	1.706637	0.007500	0.707694
-40.727402	-1.636191	1.711642	0.007475	0.707701
-40.746968	-1.637242	1.716646	0.007479	0.707692
-40.580833	-1.666528	1.721651	0.007448	0.707693
-41.378805	-1.665153	1.726656	0.007596	0.707411
-42.000688	-1.577122	1.731661	0.007711	0.707366
-41.372509	-1.684955	1.736666	0.007594	0.707375
-41.548321	-1.657337	1.741670	0.007627	0.707368
-42.127133	-1.551585	1.746675	0.007734	0.707373
-41.510262	-1.662575	1.751680	0.007619	0.707372
-41.577598	-1.651958	1.756685	0.007631	0.707370
-41.850906	-1.697610	1.761690	0.007682	0.707181
-42.678295	-1.602952	1.766694	0.007836	0.707075
-42.323056	-1.664354	1.771699	0.007769	0.707080
-42.205338	-1.686528	1.776704	0.007747	0.707078
-42.361115	-1.662362	1.781709	0.007776	0.707071
-42.148047	-1.694223	1.786714	0.007736	0.707084
-42.438779	-1.660581	1.791718	0.007790	0.707048
-43.387201	-1.639901	1.796723	0.007966	0.706750
-43.103566	-1.690951	1.801728	0.007913	0.706750
-43.639675	-1.599143	1.806733	0.008012	0.706743
-43.518167	-1.616747	1.811738	0.007990	0.706752
-43.317928	-1.656584	1.816742	0.007952	0.706744
-43.333839	-1.649964	1.821747	0.007955	0.706752
-43.459398	-1.627491	1.826752	0.007978	0.706753
-44.129869	-1.647007	1.831757	0.008102	0.706474
-44.090467	-1.668115	1.836762	0.008095	0.706446
-44.234738	-1.645608	1.841766	0.008121	0.706440
-44.393349	-1.617320	1.846771	0.008151	0.706441
-44.158728	-1.658003	1.851776	0.008107	0.706443
-44.352812	-1.627742	1.856781	0.008143	0.706435
-44.411328	-1.613025	1.861786	0.008153	0.706444
-44.585334	-1.692359	1.866790	0.008185	0.706223
-44.982097	-1.672983	1.871795	0.008259	0.706120
-44.966581	-1.672824	1.876800	0.008256	0.706127
-45.549785	-1.571720	1.881805	0.008364	0.706122
-45.333606	-1.607137	1.886810	0.008324	0.706128
-45.353058	-1.606917	1.891814	0.008327	0.706122
-45.206544	-1.632865	1.896819	0.008299	0.706123
-45.037727	-1.732352	1.901824	0.008268	0.705984
-46.028442	-1.622095	1.906829	0.008452	0.705851
-45.694572	-1.674768	1.911834	0.008389	0.705866
-45.915061	-1.639175	1.916838	0.008430	0.705859
-45.877453	-1.646331	1.921843	0.008423	0.705858
-45.938846	-1.634830	1.926848	0.008434	0.705860
-46.220604	-1.586568	1.931853	0.008486	0.705856
-46.079694	-1.762170	1.936858	0.008460	0.705554
-46.579792	-1.692438	1.941862	0.008553	0.705516
-47.034730	-1.606747	1.946867	0.008637	0.705525
-46.801695	-1.648043	1.951872	0.008593	0.705526
-46.793419	-1.652802	1.956877	0.008592	0.705520
-46.989337	-1.613324	1.961882	0.008628	0.705530
-47.109140	-1.609718	1.966886	0.008650	0.705495
-47.459140	-1.689119	1.971891	0.008715	0.705210
-47.291778	-1.719019	1.976896	0.008683	0.705210
-48.095878	-1.578332	1.981901	0.008833	0.705205
-47.855236	-1.616760	1.986906	0.008788	0.705215
-47.779128	-1.634850	1.991910	0.008773	0.705206
-47.931634	-1.604974	1.996915	0.008801	0.705212
-47.921013	-1.678276	2.001920	0.008799	0.705069

-48.672556	-1.634917	2.011917	0.008939	0.704888
-48.537301	-1.659467	2.021914	0.008913	0.704888
-48.826359	-1.607674	2.031910	0.008966	0.704889
-48.703649	-1.632743	2.041907	0.008943	0.704884
-48.790592	-1.615857	2.051904	0.008958	0.704888
-48.706645	-1.629902	2.061901	0.008942	0.704891
-48.449128	-1.677568	2.071898	0.008894	0.704888
-48.919536	-1.595191	2.081894	0.008981	0.704886
-48.658147	-1.642927	2.091891	0.008932	0.704885
-48.675529	-1.609457	2.101888	0.008934	0.704947
-47.807778	-1.634225	2.111885	0.008772	0.705210
-47.629627	-1.666733	2.121882	0.008738	0.705209
-48.052739	-1.591663	2.131878	0.008817	0.705210
-47.915330	-1.617141	2.141875	0.008791	0.705209
-48.027983	-1.598000	2.151872	0.008811	0.705208
-47.795128	-1.611610	2.161869	0.008767	0.705265
-46.868343	-1.647653	2.171866	0.008594	0.705526
-46.837524	-1.655293	2.181862	0.008588	0.705523
-47.004890	-1.625856	2.191859	0.008618	0.705523
-47.033886	-1.621630	2.201856	0.008623	0.705522
-46.585593	-1.610782	2.211853	0.008539	0.705706
-45.984722	-1.642845	2.221850	0.008427	0.705858
-46.308452	-1.587283	2.231846	0.008487	0.705855
-45.776096	-1.682426	2.241843	0.008387	0.705855
-45.861415	-1.601165	2.251840	0.008402	0.705989
-45.208220	-1.650801	2.261837	0.008280	0.706124
-45.342134	-1.625696	2.271834	0.008304	0.706128
-45.165194	-1.657713	2.281830	0.008271	0.706128
-44.677097	-1.621796	2.291827	0.008180	0.706376
-44.779374	-1.569936	2.301824	0.008198	0.706445
-44.467748	-1.626079	2.311821	0.008139	0.706444
-44.387716	-1.578164	2.321818	0.008124	0.706570
-43.820060	-1.591053	2.331814	0.008018	0.706749
-43.374180	-1.671242	2.341811	0.007934	0.706748
-43.627806	-1.626859	2.351808	0.007981	0.706748
-42.829547	-1.627117	2.361805	0.007832	0.707034
-42.960176	-1.581226	2.371802	0.007856	0.707081
-42.669215	-1.634149	2.381798	0.007801	0.707079
-42.848385	-1.536391	2.391795	0.007834	0.707213
-42.041637	-1.601310	2.401792	0.007683	0.707372
-41.748279	-1.652246	2.411789	0.007628	0.707376
-41.877012	-1.629192	2.421786	0.007651	0.707377
-41.371438	-1.562259	2.431782	0.007556	0.707693
-40.987959	-1.631710	2.441779	0.007485	0.707692
-41.123601	-1.607620	2.451776	0.007509	0.707693
-40.573813	-1.612725	2.461773	0.007406	0.707880
-40.390261	-1.581606	2.471770	0.007372	0.708009
-40.015722	-1.649385	2.481766	0.007301	0.708008
-40.332634	-1.567063	2.491763	0.007360	0.708061
-39.259367	-1.617841	2.501760	0.007159	0.708344
-39.176128	-1.632997	2.511757	0.007143	0.708344
-39.406731	-1.591475	2.521754	0.007186	0.708346
-38.689312	-1.626441	2.531750	0.007052	0.708533
-38.392283	-1.629530	2.541747	0.006996	0.708634
-38.555615	-1.599139	2.551744	0.007026	0.708638
-38.231049	-1.647084	2.561741	0.006965	0.708658
-37.771784	-1.581817	2.571738	0.006879	0.708954
-37.404974	-1.647942	2.581734	0.006810	0.708954
-37.775106	-1.584324	2.591731	0.006878	0.708950
-37.280032	-1.569891	2.601728	0.006786	0.709156
-36.866089	-1.591815	2.611725	0.006708	0.709261
-36.958070	-1.575742	2.621722	0.006724	0.709262
-36.743987	-1.537118	2.631718	0.006684	0.709416
-35.997576	-1.584283	2.641715	0.006545	0.709589
-36.119675	-1.562295	2.651712	0.006567	0.709591
-35.852663	-1.579725	2.661709	0.006517	0.709652
-35.094965	-1.593260	2.671706	0.006375	0.709896
-34.802924	-1.647541	2.681702	0.006320	0.709892
-35.105711	-1.594759	2.691699	0.006376	0.709891
-34.472136	-1.623001	2.701696	0.006257	0.710061
-34.209618	-1.592446	2.711693	0.006208	0.710217
-34.180089	-1.597988	2.721690	0.006202	0.710217
-33.932816	-1.643626	2.731686	0.006155	0.710215
-33.449167	-1.577230	2.741683	0.006065	0.710521
-33.150760	-1.627089	2.751680	0.006009	0.710529
-33.213782	-1.615356	2.761677	0.006020	0.710531
-33.150068	-1.553779	2.771674	0.006007	0.710678
-32.097608	-1.646424	2.781670	0.005811	0.710868
-32.412046	-1.592510	2.791667	0.005869	0.710865
-32.234538	-1.624657	2.801664	0.005835	0.710865
-31.734549	-1.597834	2.811661	0.005742	0.711097
-31.566871	-1.608610	2.821658	0.005710	0.711137
-31.600817	-1.604642	2.831654	0.005716	0.711133
-31.411474	-1.553166	2.841651	0.005680	0.711304
-30.519305	-1.639483	2.851648	0.005513	0.711450
-30.803013	-1.587367	2.861645	0.005566	0.711455
-30.716531	-1.587307	2.871642	0.005549	0.711486
-30.000616	-1.579566	2.881638	0.005415	0.711757
-29.823178	-1.610758	2.891635	0.005381	0.711759
-29.951918	-1.589352	2.901632	0.005405	0.711757
-29.400801	-1.558463	2.911629	0.005302	0.712016
-28.959455	-1.601191	2.921626	0.005219	0.712088
-28.838642	-1.625586	2.931622	0.005196	0.712083
-29.034390	-1.539218	2.941619	0.005232	0.712187
-27.928342	-1.640316	2.951616	0.005025	0.712379
-28.327752	-1.567741	2.961613	0.005099	0.712383
-27.987235	-1.628342	2.971610	0.005035	0.712384
-27.565892	-1.554738	2.981606	0.004956	0.712681
-27.240405	-1.601551	2.991603	0.004895	0.712705
-27.271217	-1.597910	3.001600	0.004900	0.712702
-27.032746	-1.557105	3.011597	0.004855	0.712869
-26.276364	-1.614802	3.021594	0.004714	0.713023
-26.557077	-1.566007	3.031590	0.004766	0.713022
-26.499830	-1.559247	3.041587	0.004755	0.713057
-25.391249	-1.607625	3.051584	0.004548	0.713355
-25.344502	-1.613994	3.061581	0.004538	0.713359
-25.295147	-1.625660	3.071578	0.004529	0.713355
-25.345341	-1.550238	3.081574	0.004537	0.713488
-24.527577	-1.614943	3.091571	0.004385	0.713650
-24.848485	-1.559501	3.101568	0.004444	0.713648
-24.584377	-1.596105	3.111565	0.004394	0.713669
-23.839802	-1.578385	3.121562	0.004255	0.713969
-23.841005	-1.579354	3.131558	0.004255	0.713968
-23.743342	-1.598881	3.141555	0.004236	0.713965
-23.326034	-1.577191	3.151552	0.004158	0.714157
-22.849918	-1.602855	3.161549	0.004069	0.714275
-22.841144	-1.602848	3.171546	0.004066	0.714279
-22.977956	-1.563566	3.181542	0.004091	0.714310
-22.055257	-1.579597	3.191539	0.003919	0.714606
-22.149724	-1.562495	3.201536	0.003936	0.714607
-21.958525	-1.596089	3.211533	0.003900	0.714609
-21.657212	-1.551435	3.221530	0.003843	0.714805
-21.231727	-1.576366	3.231526	0.003763	0.714907
-21.075173	-1.605047	3.241523	0.003734	0.714907
-21.019454	-1.587017	3.251520	0.003723	0.714963
-20.358357	-1.569925	3.261517	0.003599	0.715232
-20.227588	-1.591806	3.271514	0.003574	0.715236
-20.434980	-1.555808	3.281510	0.003612	0.715235
-19.706223	-1.564271	3.291507	0.003476	0.715477
-19.305406	-1.602964	3.301504	0.003401	0.715543
-19.160391	-1.628130	3.311501	0.003373	0.715545
-19.252160	-1.602640	3.321498	0.003390	0.715564
-18.629651	-1.552524	3.331494	0.003274	0.715884
-18.241814	-1.622325	3.341491	0.003201	0.715884
-18.539058	-1.570441	3.351488	0.003256	0.715883
-18.139709	-1.591024	3.361485	0.003181	0.715984
-17.445801	-1.640047	3.371482	0.003051	0.716133
-17.769278	-1.582544	3.381478	0.003111	0.716134
-17.688928	-1.592875	3.391475	0.003095	0.716142
-16.974765	-1.566285	3.401472	0.002962	0.716448
-16.720685	-1.610955	3.411469	0.002914	0.716450
-16.901128	-1.579879	3.421466	0.002947	0.716449
-16.278262	-1.587058	3.431462	0.002830	0.716656
-15.927339	-1.598044	3.441459	0.002764	0.716759
-16.037181	-1.580810	3.451456	0.002784	0.716755
-15.941579	-1.555984	3.461453	0.002766	0.716839
-15.137445	-1.574492	3.471450	0.002616	0.717087
-15.132824	-1.575829	3.481446	0.002614	0.717087
-14.931715	-1.613984	3.491443	0.002576	0.717083
-14.338581	-1.596045	3.501440	0.002465	0.717329
-14.083442	-1.617464	3.511437	0.002417	0.717377
-14.061002	-1.619683	3.521434	0.002413	0.717382
-13.994638	-1.600677	3.531430	0.002400	0.717444
-13.389523	-1.578834	3.541427	0.002287	0.717701
-13.337787	-1.590264	3.551424	0.002276	0.717698
-13.042395	-1.641890	3.561421	0.002221	0.717701
-12.785843	-1.578400	3.571418	0.002172	0.717917
-11.703102	-1.723270	3.581414	0.001970	0.718013
-11.685212	-1.727209	3.591411	0.001967	0.718013
-11.654053	-1.732601	3.601408	0.001960	0.718014
-11.596401	-1.697533	3.611405	0.001949	0.718105
-10.662034	-1.738276	3.621402	0.001774	0.718354
-10.646006	-1.741606	3.631398	0.001771	0.718354
-10.946658	-1.688612	3.641395	0.001826	0.718354
-10.931414	-1.690813	3.651392	0.001823	0.718356
-9.971432	-1.716510	3.661389	0.001644	0.718644
-10.077932	-1.697265	3.671386	0.001663	0.718645
-9.658941	-1.771809	3.681382	0.001584	0.718646
-10.019910	-1.697145	3.691379	0.001651	0.718668
-8.962548	-1.737461	3.701376	0.001454	0.718961
-9.024522	-1.726503	3.711373	0.001465	0.718962
-8.889092	-1.749276	3.721370	0.001439	0.718965
-9.117902	-1.668275	3.731366	0.001481	0.719046
-8.136726	-1.729298	3.741363	0.001298	0.719271
-8.017008	-1.752323	3.751360	0.001275	0.719269
-8.002792	-1.754576	3.761357	0.001272	0.719270
-8.228295	-1.628326	3.771354	0.001313	0.719441
-7.031103	-1.762722	3.781350	0.001090	0.719598
-7.613824	-1.657239	3.791347	0.001198	0.719602
-7.241522	-1.707642	3.801344	0.001128	0.719634
-6.668044	-1.677111	3.811341	0.001021	0.719897
-6.216486	-1.758162	3.821338	0.000936	0.719896
-6.357859	-1.733420	3.831334	0.000962	0.719897
-5.965380	-1.713893	3.841331	0.000888	0.720074
-5.370548	-1.746967	3.851328	0.000777	0.720218
-5.479778	-1.726601	3.861325	0.000797	0.720221
-5.331350	-1.752675	3.871322	0.000768	0.720223
-4.609589	-1.754109	3.881318	0.000634	0.720474
-4.642855	-1.716461	3.891315	0.000639	0.720538
-4.465211	-1.749166	3.901312	0.000606	0.720536
-4.649235	-1.694000	3.911309	0.000639	0.720582
-3.781600	-1.699374	3.921306	0.000477	0.720876
-3.734566	-1.707748	3.931302	0.000468	0.720877
-3.629822	-1.725604	3.941299	0.000448	0.720880
-3.238772	-1.723649	3.951296	0.000374	0.721021
-3.214264	-1.677746	3.961293	0.000369	0.721121
-2.814373	-1.748716	3.971290	0.000294	0.721123
-3.019431	-1.655726	3.981286	0.000332	0.721235
-2.352443	-1.672019	3.991283	0.000207	0.721437
-2.260305	-1.688980	4.001280	0.000190	0.721437
-2.242963	-1.662049	4.011277	0.000186	0.721497
-1.774901	-1.618856	4.021274	0.000098	0.721747
-1.445151	-1.677809	4.031270	0.000036	0.721748
-1.679738	-1.608470	4.041267	0.000079	0.721803
-1.388595	-1.522934	4.051264	0.000024	0.722074
-1.274653	-1.543140	4.061261	0.000003	0.722075
-1.148189	-1.486023	4.071258	-0.000021	0.722232
-0.833657	-1.470535	4.081254	-0.000081	0.722373
-0.812514	-1.468644	4.091251	-0.000085	0.722386
-0.711161	-1.331197	4.101248	-0.000104	0.722692
-0.915055	-1.293535	4.111245	-0.000067	0.722695
-0.840922	-1.160459	4.121242	-0.000082	0.722983
-0.662017	-1.177208	4.131238	-0.000115	0.723014
-0.594203	-1.022611	4.141235	-0.000129	0.723342
-0.421388	-1.020368	4.151232	-0.000161	0.723408
-0.318431	-0.922506	4.161229	-0.000181	0.723636
-0.438204	-0.814271	4.171226	-0.000159	0.723808
-0.327854	-0.758037	4.181222	-0.000181	0.723957
-0.415633	-0.588291	4.191219	-0.000165	0.724260
-0.353288	-0.505258	4.201216	-0.000177	0.724445
-0.592507	-0.349904	4.211213	-0.000133	0.724667
-0.337064	-0.282060	4.221210	-0.000181	0.724890
-0.264056	-0.133266	4.231206	-0.000196	0.725207
-0.270674	-0.007968	4.241203	-0.000195	0.725451
0.000000	0.088920	4.251200	-0.000246	0.725736

-0.112114	0.728668	4.256205	-0.000226	0.726946
-0.053052	2.000759	4.261210	-0.000238	0.729444
0.251062	3.806629	4.266214	-0.000296	0.733052
0.512690	6.181082	4.271219	-0.000346	0.737721
0.672095	9.082340	4.276224	-0.000378	0.743331
0.948438	12.452940	4.281229	-0.000432	0.749827
1.450171	16.229564	4.286234	-0.000528	0.757103
1.484521	20.483058	4.291238	-0.000538	0.765040
1.877422	25.093695	4.296243	-0.000614	0.773667
2.232241	30.061780	4.301248	-0.000684	0.782834
2.351213	35.425404	4.306253	-0.000710	0.792528
2.833954	41.034490	4.311258	-0.000804	0.802653
3.280230	46.958332	4.316262	-0.000891	0.813188
4.001800	53.122785	4.321267	-0.001029	0.824087
4.291951	59.635663	4.326272	-0.001088	0.835305
4.668577	66.337440	4.331277	-0.001163	0.846717
5.507150	73.205874	4.336282	-0.001324	0.858386
5.800425	80.361871	4.341286	-0.001383	0.870210
6.515546	87.635241	4.346291	-0.001521	0.882184
7.082045	95.103942	4.351296	-0.001632	0.894265
7.522082	102.750193	4.356301	-0.001719	0.906428
8.037046	110.529597	4.361306	-0.001820	0.918655
8.390662	118.440612	4.366310	-0.001892	0.930879
9.346123	126.372808	4.371315	-0.002075	0.943135
9.988180	134.473561	4.376320	-0.002200	0.955401
10.863505	142.619543	4.381325	-0.002369	0.967637
11.253461	150.933950	4.386330	-0.002447	0.979842
11.734584	159.317399	4.391334	-0.002542	0.992017
12.994509	167.611679	4.396339	-0.002782	1.004110
14.073516	175.989937	4.401344	-0.002989	1.016131
15.099089	184.423322	4.406349	-0.003186	1.028074
15.663692	192.989333	4.411354	-0.003297	1.039952
16.332971	201.549783	4.416358	-0.003427	1.051712
17.195775	210.120178	4.421363	-0.003594	1.063399
17.688477	218.777169	4.426368	-0.003691	1.074989
18.614368	227.349019	4.431373	-0.003870	1.086441
19.581610	235.947980	4.436378	-0.004056	1.097817
20.381550	244.569369	4.441382	-0.004211	1.109069
21.059009	253.218802	4.446387	-0.004343	1.120215
21.742563	261.865127	4.451392	-0.004476	1.131249
22.671804	270.466156	4.456397	-0.004655	1.142172
23.208053	279.170156	4.461402	-0.004760	1.153034
23.974764	287.773591	4.466406	-0.004909	1.163721
25.065640	296.338492	4.471411	-0.005118	1.174330
25.574984	304.974932	4.476416	-0.005219	1.184810
26.459584	313.558697	4.481421	-0.005389	1.195212
27.378033	322.104876	4.486426	-0.005566	1.205486
27.928727	330.713443	4.491430	-0.005675	1.215673
28.813360	339.257109	4.496435	-0.005845	1.225765
29.280665	347.877686	4.501440	-0.005938	1.235782
30.046719	356.395667	4.506445	-0.006087	1.245658
30.757110	364.940091	4.511450	-0.006225	1.255476
31.254743	373.474553	4.516454	-0.006323	1.265166
32.347809	381.940863	4.521459	-0.006532	1.274818
32.780970	390.463577	4.526464	-0.006619	1.284336
33.668271	398.920200	4.531469	-0.006790	1.293795
34.180124	407.415296	4.536474	-0.006891	1.303159
34.757488	415.975170	4.541478	-0.007004	1.312537
35.314770	424.458744	4.546483	-0.007114	1.321763
35.861567	432.877331	4.551488	-0.007222	1.330854
36.740888	441.242187	4.556493	-0.007391	1.339885
37.154660	449.686934	4.561498	-0.007474	1.348857
37.232251	458.161961	4.566502	-0.007494	1.357743
38.016111	466.498143	4.571507	-0.007646	1.366549
38.672721	474.865412	4.576512	-0.007774	1.375308
39.355292	483.217384	4.581517	-0.007907	1.384001
39.847893	491.619688	4.586522	-0.008004	1.392658
40.197472	499.984097	4.591526	-0.008075	1.401199
40.847663	508.308435	4.596531	-0.008202	1.409698
41.441907	516.635004	4.601536	-0.008318	1.418139
42.111266	524.939506	4.606541	-0.008448	1.426520
42.422031	533.326796	4.611546	-0.008512	1.434875
42.989532	541.617027	4.616550	-0.008623	1.443128
43.694088	549.919912	4.621555	-0.008760	1.451368
44.156985	558.234833	4.626560	-0.008852	1.459535
44.442329	566.589955	4.631565	-0.008911	1.467666
45.012257	574.925867	4.636570	-0.009023	1.475779
45.485089	583.193240	4.641574	-0.009116	1.483766
46.072431	591.456716	4.646579	-0.009231	1.491725
46.333194	599.757528	4.651584	-0.009286	1.499626
47.122253	607.963829	4.656589	-0.009438	1.507478
47.977262	616.197730	4.661594	-0.009603	1.515325
48.657554	624.411231	4.666598	-0.009735	1.523085
49.449001	632.655716	4.671603	-0.009888	1.530852
49.887918	640.937443	4.676608	-0.009976	1.538560
50.372555	649.190841	4.681613	-0.010071	1.546211
50.849896	657.494667	4.686618	-0.010166	1.553868
51.254223	665.731777	4.691622	-0.010247	1.561417
51.620264	673.994559	4.696627	-0.010321	1.568947
51.846554	682.263438	4.701632	-0.010369	1.576426
52.502919	690.449007	4.706637	-0.010496	1.583857
53.075223	698.673342	4.711642	-0.010609	1.591275
53.480882	706.893081	4.716646	-0.010690	1.598631
54.200615	715.072809	4.721651	-0.010829	1.605963
54.770890	723.296443	4.726656	-0.010941	1.613278
55.286677	731.500378	4.731661	-0.011043	1.620535
55.995097	739.704992	4.736666	-0.011180	1.627787
56.523164	747.966846	4.741670	-0.011284	1.635032
56.978619	756.162428	4.746675	-0.011375	1.642177
57.559149	764.341779	4.751680	-0.011488	1.649294
58.193681	772.530292	4.756685	-0.011612	1.656395
58.739596	780.715407	4.761690	-0.011719	1.663451
59.026095	788.926452	4.766694	-0.011778	1.670464
59.694747	797.101041	4.771699	-0.011909	1.677468
60.044895	805.282438	4.776704	-0.011979	1.684407
60.388461	813.491567	4.781709	-0.012049	1.691338
60.756937	821.705946	4.786714	-0.012123	1.698249
61.081432	829.873736	4.791718	-0.012189	1.705088
61.368295	838.111960	4.796723	-0.012248	1.711952
61.670362	846.287772	4.801728	-0.012310	1.718739
61.975868	854.437498	4.806733	-0.012373	1.725479
62.623571	862.592275	4.811738	-0.012499	1.732240
62.596251	870.807972	4.816742	-0.012499	1.738939
63.076510	878.945093	4.821747	-0.012594	1.745612
63.605069	887.104001	4.826752	-0.012698	1.752283
64.181183	895.235166	4.831757	-0.012811	1.758913
64.536598	903.389795	4.836762	-0.012883	1.765509
64.927125	911.550493	4.841766	-0.012961	1.772089
65.283171	919.723184	4.846771	-0.013033	1.778650
65.720390	927.855556	4.851776	-0.013120	1.785165
65.931845	936.077828	4.856781	-0.013165	1.791699
66.553241	944.218836	4.861786	-0.013286	1.798196
66.739376	952.366146	4.866790	-0.013327	1.804621
67.049685	960.524307	4.871795	-0.013390	1.811046
67.175711	968.693123	4.876800	-0.013419	1.817436
67.347969	976.834234	4.881805	-0.013457	1.823786
67.778342	984.963157	4.886810	-0.013542	1.830136
68.074960	993.099801	4.891814	-0.013603	1.836454
68.631818	1001.204681	4.896819	-0.013712	1.842756
68.944669	1009.347758	4.901824	-0.013776	1.849038
69.453751	1017.465045	4.906829	-0.013877	1.855301
70.046449	1025.579195	4.911834	-0.013992	1.861550
70.187000	1033.738984	4.916838	-0.014024	1.867760
70.521359	1041.921726	4.921843	-0.014092	1.873990
71.082392	1049.992144	4.926848	-0.014202	1.880140
71.280127	1058.133377	4.931853	-0.014244	1.886282
71.284755	1066.330705	4.936858	-0.014251	1.892423
71.536248	1074.444350	4.941862	-0.014303	1.898511
72.117094	1082.523845	4.946867	-0.014417	1.904590
72.440538	1090.658979	4.951872	-0.014483	1.910662
72.414010	1098.827992	4.956877	-0.014483	1.916701
72.942879	1106.913017	4.961882	-0.014587	1.922721
73.255990	1115.024928	4.966886	-0.014651	1.928718
73.853413	1123.123395	4.971891	-0.014768	1.934717
74.261084	1131.224717	4.976896	-0.014850	1.940680
74.680828	1139.334913	4.981901	-0.014933	1.946631
74.911596	1147.531406	4.986906	-0.014982	1.952606
75.246061	1155.625573	4.991910	-0.015050	1.958500
75.654135	1163.713049	4.996915	-0.015131	1.964380
75.651838	1171.867766	5.001920	-0.015136	1.970246
75.951107	1179.982180	5.006925	-0.015198	1.976098
76.438501	1188.062712	5.011930	-0.015294	1.981929
76.678936	1196.165643	5.016934	-0.015344	1.987732
76.912945	1204.319380	5.021939	-0.015393	1.993553
77.215915	1212.400037	5.026944	-0.015455	1.999313
77.633984	1220.468623	5.031949	-0.015539	2.005060
77.899222	1228.590230	5.036954	-0.015594	2.010811
78.160181	1236.707046	5.041958	-0.015648	2.016543
78.756219	1244.770933	5.046963	-0.015764	2.022255
78.854051	1252.910804	5.051968	-0.015788	2.027954
78.999592	1261.069335	5.056973	-0.015821	2.033654
79.606677	1269.124288	5.061978	-0.015939	2.039313
79.854324	1277.200784	5.066982	-0.015991	2.044935
79.977662	1285.336509	5.071987	-0.016020	2.050569
80.409700	1293.422285	5.076992	-0.016106	2.056185
80.851365	1301.487727	5.081997	-0.016193	2.061773
81.136599	1309.609449	5.087002	-0.016252	2.067368
81.155448	1317.747923	5.092006	-0.016261	2.072932
81.760859	1325.817096	5.097011	-0.016379	2.078493
81.826360	1333.928085	5.102016	-0.016397	2.084014
81.902092	1342.031043	5.107021	-0.016417	2.089516
82.461041	1350.128065	5.112026	-0.016526	2.095047
82.484767	1358.230192	5.117030	-0.016536	2.100514
82.976609	1366.297328	5.122035	-0.016633	2.105989
83.152277	1374.446464	5.127040	-0.016672	2.111474
83.499676	1382.554321	5.132045	-0.016742	2.116934
83.879904	1390.590151	5.137050	-0.016818	2.122335
84.041443	1398.674482	5.142054	-0.016854	2.127733
84.583704	1406.748993	5.147059	-0.016960	2.133147
84.883534	1414.826636	5.152064	-0.017022	2.138527
85.208994	1422.879558	5.157069	-0.017088	2.143879
85.470843	1430.989004	5.162074	-0.017142	2.149249
85.671300	1439.097532	5.167078	-0.017185	2.154599
85.868264	1447.191610	5.172083	-0.017227	2.159926
86.039703	1455.284149	5.177088	-0.017265	2.165236
86.273175	1463.361044	5.182093	-0.017314	2.170529
86.709366	1471.454228	5.187098	-0.017400	2.175838
86.872049	1479.524050	5.192102	-0.017436	2.181094
87.178932	1487.614978	5.197107	-0.017499	2.186364
87.448780	1495.720275	5.202112	-0.017555	2.191628
87.496437	1503.833783	5.207117	-0.017569	2.196863
88.000754	1511.860179	5.212122	-0.017669	2.202072
88.330528	1519.908166	5.217126	-0.017736	2.207266
88.501861	1528.017938	5.222131	-0.017773	2.212473
88.775087	1536.097391	5.227136	-0.017829	2.217658
89.100109	1544.142578	5.232141	-0.017895	2.222813
89.381236	1552.249479	5.237146	-0.017953	2.227992
89.548444	1560.351244	5.242150	-0.017990	2.233145
90.002367	1568.400646	5.247155	-0.018080	2.238279
90.161691	1576.486980	5.252160	-0.018115	2.243398
90.641420	1584.524904	5.257165	-0.018210	2.248502
90.759960	1592.658105	5.262170	-0.018238	2.253624
91.119464	1600.703868	5.267174	-0.018310	2.258700
91.276792	1608.797320	5.272179	-0.018345	2.263777
91.660828	1616.854848	5.277184	-0.018422	2.268840
92.074733	1625.003308	5.282189	-0.018505	2.273950
92.600232	1633.024196	5.287194	-0.018608	2.278979
92.770816	1641.083955	5.292198	-0.018645	2.283991
93.130845	1649.144271	5.297203	-0.018718	2.289008
93.509799	1657.220436	5.302208	-0.018794	2.294026
93.552820	1665.313046	5.307213	-0.018808	2.299014
93.987752	1673.361844	5.312218	-0.018894	2.303997
94.079134	1681.443371	5.317222	-0.018917	2.308961
94.292007	1689.556123	5.322227	-0.018962	2.313944
94.612387	1697.597097	5.327232	-0.019027	2.318880
94.812400	1705.643401	5.332237	-0.019070	2.323800
95.385193	1713.688733	5.337242	-0.019182	2.328739
95.389042	1721.799628	5.342246	-0.019188	2.333661
95.581210	1729.875482	5.347251	-0.019229	2.338566
96.021533	1737.918204	5.352256	-0.019317	2.343462
96.191444	1745.992411	5.357261	-0.019354	2.348344
96.660236	1754.090111	5.362266	-0.019447	2.353254
97.063331	1762.103059	5.367270	-0.019527	2.358098
97.345815	1770.175903	5.372275	-0.019586	2.362958
97.471156	1778.246495	5.377280	-0.019614	2.367793
97.862530	1786.320410	5.382285	-0.019693	2.372643
97.974863	1794.417379	5.387290	-0.019719	2.377473
98.232266	1802.457275	5.392294	-0.019773	2.382272
98.670660	1810.508553	5.397299	-0.019860	2.387082
98.680519	1818.629470	5.402304	-0.019867	2.391889
98.968346	1826.682266	5.407309	-0.019926	2.396669
99.229622	1834.738444	5.412314	-0.019981	2.401438
99.652725	1842.764572	5.417318	-0.020065	2.406194
99.753462	1850.856920	5.422323	-0.020089	2.410953
100.141534	1858.934650	5.427328	-0.020167	2.415717
100.223424	1866.998119	5.432333	-0.020188	2.420439
100.666927	1875.038092	5.437338	-0.020276	2.425167
100.918578	1883.108418	5.442342	-0.020328	2.429888
101.317295	1891.241849	5.447347	-0.020408	2.434647
101.859162	1899.217503	5.452352	-0.020514	2.439317
101.992795	1907.285998	5.457357	-0.020545	2.444000
102.389561	1915.325758	5.462362	-0.020624	2.448678
102.746335	1923.376655	5.467366	-0.020696	2.453350
103.098447	1931.438595	5.472371	-0.020767	2.458019
103.263740	1939.500035	5.477376	-0.020804	2.462665
103.552867	1947.559277	5.482381	-0.020863	2.467310
103.744600	1955.667618	5.487386	-0.020904	2.471967
104.029883	1963.706203	5.492390	-0.020963	2.476583
104.267916	1971.771050	5.497395	-0.021013	2.481201
104.687217	1979.798459	5.502400	-0.021096	2.485803
104.746044	1987.881157	5.507405	-0.021113	2.490401
104.952832	1995.977039	5.512410	-0.021157	2.495008
105.159645	2004.006069	5.517414	-0.021201	2.499570
105.583122	2012.045164	5.522419	-0.021285	2.504144
105.681968	2020.146333	5.527424	-0.021309	2.508722
106.216330	2028.200227	5.532429	-0.021414	2.513296
106.821371	2036.247829	5.537434	-0.021532	2.517863
106.863336	2044.279069	5.542438	-0.021546	2.522372
107.134330	2052.346993	5.547443	-0.021602	2.526910
107.486623	2060.387061	5.552448	-0.021673	2.531430
107.757919	2068.447311	5.557453	-0.021729	2.535947
107.950234	2076.516476	5.562458	-0.021770	2.540456
108.166093	2084.543440	5.567462	-0.021816	2.544935
108.645484	2092.595664	5.572467	-0.021911	2.549438
108.772533	2100.685437	5.577472	-0.021940	2.553930
108.982658	2108.707547	5.582477	-0.021984	2.558382
109.336927	2116.751847	5.587482	-0.022056	2.562848
109.692880	2124.779015	5.592486	-0.022128	2.567298
109.927147	2132.857264	5.597491	-0.022177	2.571759
110.032307	2140.965668	5.602496	-0.022202	2.576220
110.465668	2148.965441	5.607501	-0.022288	2.580636
110.777596	2157.029828	5.612506	-0.022352	2.585072
110.969649	2165.087839	5.617510	-0.022393	2.589488
111.111305	2173.356792	5.622515	-0.022425	2.594009
111.319825	2181.358485	5.627520	-0.022469	2.598380
111.436051	2189.370646	5.632525	-0.022496	2.602744
111.888894	2197.361598	5.637530	-0.022586	2.607111
111.982086	2205.401734	5.642534	-0.022609	2.611474
112.157220	2213.461956	5.647539	-0.022647	2.615846
112.417955	2221.481766	5.652544	-0.022701	2.620194
112.561613	2229.493330	5.657549	-0.022733	2.624522
112.783685	2237.574998	5.662554	-0.022780	2.628887
112.936208	2245.628519	5.667558	-0.022814	2.633224
113.466153	2253.638435	5.672563	-0.022918	2.637556
113.606943	2261.686956	5.677568	-0.022950	2.641876
113.815720	2269.727245	5.682573	-0.022995	2.646188
114.229861	2277.776675	5.687578	-0.023077	2.650512
114.341913	2285.854792	5.692582	-0.023104	2.654824
114.638288	2293.890408	5.697587	-0.023164	2.659119
114.774760	2301.934007	5.702592	-0.023195	2.663400
115.032239	2309.967057	5.707597	-0.023249	2.667677
115.450642	2318.063810	5.712602	-0.023332	2.671991
115.533142	2326.123079	5.717606	-0.023353	2.676257
115.751511	2334.151558	5.722611	-0.023399	2.680508
115.849682	2342.187307	5.727616	-0.023423	2.684749
115.915499	2350.230237	5.732621	-0.023441	2.688984
116.410349	2358.293015	5.737626	-0.023538	2.693251
116.505249	2366.342584	5.742630	-0.023562	2.697478
116.453587	2374.413523	5.747635	-0.023557	2.701701
116.675985	2382.439655	5.752640	-0.023604	2.705911
117.121450	2390.454077	5.757645	-0.023693	2.710122
117.541785	2398.537596	5.762650	-0.023777	2.714361
117.416789	2406.591085	5.767654	-0.023759	2.718544
117.842109	2414.582844	5.772659	-0.023844	2.722723
118.113592	2422.649423	5.777664	-0.023900	2.726924
118.277664	2430.700359	5.782669	-0.023936	2.731104
118.485858	2438.787495	5.787674	-0.023980	2.735299
118.638453	2446.805420	5.792678	-0.024014	2.739449
118.815785	2454.844185	5.797683	-0.024052	2.743604
119.200570	2462.874989	5.802688	-0.024130	2.747762
119.379995	2470.985562	5.807693	-0.024169	2.751941
119.530326	2479.081564	5.812698	-0.024202	2.756105
119.656757	2487.067114	5.817702	-0.024231	2.760205
119.994451	2495.060586	5.822707	-0.024299	2.764316
120.153103	2503.136664	5.827712	-0.024335	2.768451
120.061966	2511.198400	5.832717	-0.024323	2.772559
120.506585	2519.218692	5.837722	-0.024411	2.776671
120.806337	2527.217649	5.842726	-0.024473	2.780757
121.030660	2535.247785	5.847731	-0.024520	2.784849
121.136759	2543.327628	5.852736	-0.024545	2.788953
121.492678	2551.368255	5.857741	-0.024617	2.793045
121.745311	2559.405037	5.862746	-0.024670	2.797124
121.914395	2567.423754	5.867750	-0.024707	2.801183
122.334636	2575.451868	5.872755	-0.024790	2.805255
122.724629	2583.487927	5.877760	-0.024868	2.809323
123.000033	2591.549662	5.882765	-0.024925	2.813391
122.941601	2599.645997	5.887770	-0.024920	2.817452
123.296902	2607.653588	5.892774	-0.024992	2.821486
123.705633	2615.665483	5.897779	-0.025073	2.825520
123.629010	2623.749502	5.902784	-0.025064	2.829556
123.763697	2631.842844	5.907789	-0.025095	2.833603
124.077039	2639.862307	5.912794	-0.025159	2.837618
124.055272	2647.902513	5.917798	-0.025160	2.841618
124.421979	2655.911231	5.922803	-0.025234	2.845619
124.763789	2663.929843	5.927808	-0.025303	2.849618
124.851611	2671.995564	5.932813	-0.025325	2.853620
125.124367	2680.035379	5.937818	-0.025381	2.857614
125.462693	2688.050131	5.942822	-0.025450	2.861593
125.823103	2696.080080	5.947827	-0.025522	2.865576
125.852793	2704.152833	5.952832	-0.025534	2.869556
126.196291	2712.216883	5.957837	-0.025603	2.873543
126.441847	2720.247343	5.962842	-0.025654	2.877503
126.562828	2728.270454	5.967846	-0.025682	2.881447
126.723007	2736.307274	5.972851	-0.025718	2.885395
127.018476	2744.347159	5.977856	-0.025778	2.889346
127.215555	2752.384218	5.982861	-0.025820	2.893284
127.371956	2760.456060	5.987866	-0.025855	2.897233
127.474848	2768.482754	5.992870	-0.025880	2.901150
127.886676	2776.489427	5.997875	-0.025962	2.905070
127.954595	2784.564367	6.002880	-0.025980	2.908998
128.219553	2792.661392	6.007885	-0.026035	2.912943
128.357467	2800.749354	6.012890	-0.026066	2.916871
128.465344	2808.714141	6.017894	-0.026092	2.920733
128.774329	2816.702398	6.022899	-0.026155	2.924611
129.406420	2824.712688	6.027904	-0.026278	2.928512
129.599120	2832.772897	6.032909	-0.026319	2.932409
129.770580	2840.854039	6.037914	-0.026357	2.936309
129.991404	2848.839310	6.042918	-0.026403	2.940161
130.342250	2856.858791	6.047923	-0.026474	2.944030
130.547111	2864.917867	6.052928	-0.026518	2.947906
130.678094	2872.980006	6.057933	-0.026548	2.951775
131.065583	2881.035550	6.062938	-0.026625	2.955648
131.000464	2889.055186	6.067942	-0.026619	2.959476
131.159754	2897.083951	6.072947	-0.026654	2.963315
131.477713	2905.120603	6.077952	-0.026719	2.967161
131.836680	2913.106346	6.082957	-0.026791	2.970979
132.061734	2921.193143	6.087962	-0.026838	2.974834
132.247971	2929.213744	6.092966	-0.026879	2.978650
132.502523	2937.259861	6.097971	-0.026931	2.982477
132.738262	2945.321757	6.102976	-0.026981	2.986306
132.747393	2953.351468	6.107981	-0.026988	2.990103
133.163535	2961.420355	6.112986	-0.027071	2.993934
133.098334	2969.440784	6.117990	-0.027064	2.997713
133.273454	2977.456532	6.122995	-0.027103	3.001497
133.615961	2985.478126	6.128000	-0.027172	3.005288
133.863837	2993.489407	6.133005	-0.027223	3.009064
133.952382	3001.588216	6.138010	-0.027245	3.012868
134.101354	3009.608317	6.143014	-0.027279	3.016634
134.382928	3017.639996	6.148019	-0.027337	3.020407
134.605353	3025.654638	6.153024	-0.027384	3.024164
134.799852	3033.668899	6.158029	-0.027425	3.027915
135.387858	3041.721927	6.163034	-0.027540	3.031699
135.656259	3049.785663	6.168038	-0.027596	3.035467
135.602004	3057.815114	6.173043	-0.027591	3.039199
135.828378	3065.854284	6.178048	-0.027639	3.042944
136.119768	3073.858390	6.183053	-0.027699	3.046672
136.461953	3081.915758	6.188058	-0.027768	3.050422
136.549638	3089.960820	6.193062	-0.027790	3.054150
136.888669	3097.976429	6.198067	-0.027858	3.057871
137.026840	3106.024609	6.203072	-0.027890	3.061594
137.145256	3114.054877	6.208077	-0.027917	3.065302
137.441457	3122.095093	6.213082	-0.027978	3.069019
137.922895	3130.157574	6.218086	-0.028073	3.072751
138.104515	3138.221180	6.223091	-0.028112	3.076464
138.281386	3146.204571	6.228096	-0.028151	3.080136
138.547248	3154.204242	6.233101	-0.028206	3.083815
138.813627	3162.254501	6.238106	-0.028261	3.087513
138.888986	3170.292166	6.243110	-0.028280	3.091191
139.116264	3178.353556	6.248115	-0.028328	3.094883
139.203179	3186.364165	6.253120	-0.028350	3.098541
139.285857	3194.376490	6.258125	-0.028371	3.102196
139.773670	3202.414014	6.263130	-0.028467	3.105876
139.966043	3210.440696	6.268134	-0.028508	3.109533
140.058132	3218.511024	6.273139	-0.028531	3.113201
140.316551	3226.548869	6.278144	-0.028585	3.116857
140.456621	3234.548740	6.283149	-0.028616	3.120487
140.902941	3242.543502	6.288154	-0.028705	3.124124
141.134834	3250.600156	6.293158	-0.028753	3.127775
141.580340	3258.651468	6.298163	-0.028842	3.131428
141.838966	3266.697587	6.303168	-0.028896	3.135067
142.109291	3274.702089	6.308173	-0.028951	3.138683
142.367071	3282.754010	6.313178	-0.029005	3.142316
142.499384	3290.784575	6.318182	-0.029035	3.145929
142.745786	3298.804929	6.323187	-0.029086	3.149539
142.967114	3306.893521	6.328192	-0.029133	3.153174
143.003324	3314.922382	6.333197	-0.029145	3.156770
143.319489	3322.929004	6.338202	-0.029210	3.160364
143.700282	3330.884080	6.343206	-0.029286	3.163934
143.834168	3338.917768	6.348211	-0.029317	3.167524
144.097382	3347.004221	6.353216	-0.029371	3.171139
144.114864	3355.065501	6.358221	-0.029380	3.174728
144.421648	3363.087689	6.363226	-0.029443	3.178308
144.757100	3371.088897	6.368230	-0.029511	3.181875
144.882623	3379.135587	6.373235	-0.029539	3.185451
144.932952	3387.183779	6.378240	-0.029554	3.189019
145.184038	3395.179500	6.383245	-0.029607	3.192569
145.449060	3403.273361	6.388250	-0.029661	3.196158
145.536735	3411.257521	6.393254	-0.029683	3.199688
145.932508	3419.251752	6.398259	-0.029762	3.203231
146.169498	3427.315450	6.403264	-0.029812	3.206794
146.273215	3435.353289	6.408269	-0.029837	3.210337
146.340014	3443.422731	6.413274	-0.029855	3.213887
146.683278	3451.403984	6.418278	-0.029924	3.217407
146.942764	3459.462548	6.423283	-0.029978	3.220953
147.028534	3467.482258	6.428288	-0.030000	3.224471
147.091810	3475.525013	6.433293	-0.030017	3.227994
147.588184	3483.579022	6.438298	-0.030115	3.231536
147.604571	3491.650365	6.443302	-0.030123	3.235062
147.914518	3499.629491	6.448307	-0.030187	3.238555
148.384520	3507.616878	6.453312	-0.030280	3.242056
148.492889	3515.617197	6.458317	-0.030305	3.245543
148.817104	3523.647901	6.463322	-0.030371	3.249048
148.927906	3531.704962	6.468326	-0.030397	3.252553
148.979448	3539.776947	6.473331	-0.030412	3.256057
149.185623	3547.771402	6.478336	-0.030456	3.259531
149.625112	3555.741575	6.483341	-0.030543	3.262999
149.824480	3563.816787	6.488346	-0.030586	3.266500
149.905653	3571.858773	6.493350	-0.030607	3.269978
150.254939	3579.919702	6.498355	-0.030677	3.273471
150.551340	3587.947853	6.503360	-0.030738	3.276944
150.780228	3595.942198	6.508365	-0.030786	3.280396
151.138336	3603.960259	6.513370	-0.030858	3.283859
151.267474	3611.999636	6.518374	-0.030888	3.287320
151.720237	3620.032235	6.523379	-0.030978	3.290786
151.832590	3628.125240	6.528384	-0.031004	3.294261
151.775777	3636.129733	6.533389	-0.030999	3.297688
151.955560	3644.171729	6.538394	-0.031038	3.301136
152.168015	3652.138209	6.543398	-0.031083	3.304550
152.448460	3660.181585	6.548403	-0.031141	3.307996
152.638247	3668.258389	6.553408	-0.031182	3.311449
153.107046	3676.249349	6.558413	-0.031274	3.314872
153.194886	3684.287648	6.563418	-0.031296	3.318298
153.246484	3692.298576	6.568422	-0.031311	3.321707
153.697834	3700.300929	6.573427	-0.031401	3.325123
153.637944	3708.372133	6.578432	-0.031395	3.328547
153.813657	3716.379388	6.583437	-0.031433	3.331948
154.130084	3724.449716	6.588442	-0.031498	3.335378
154.323196	3732.441088	6.593446	-0.031539	3.338766
154.492066	3740.476046	6.598451	-0.031576	3.342168
154.962706	3748.472333	6.603456	-0.031669	3.345562
155.003284	3756.510571	6.608461	-0.031682	3.348954
155.126543	3764.620254	6.613466	-0.031711	3.352376
155.344036	3772.618102	6.618470	-0.031757	3.355750
155.625923	3780.616336	6.623475	-0.031815	3.359124
156.046914	3788.628641	6.628480	-0.031899	3.362505
156.048746	3796.659115	6.633485	-0.031905	3.365875
156.208280	3804.704269	6.638490	-0.031940	3.369254
156.372919	3812.757892	6.643494	-0.031976	3.372633
156.531874	3820.800005	6.648499	-0.032011	3.376004
156.833841	3828.791005	6.653504	-0.032073	3.379354
156.896010	3836.813410	6.658509	-0.032090	3.382706
157.105825	3844.871755	6.663514	-0.032135	3.386075
157.330075	3852.862810	6.668518	-0.032182	3.389413
157.650047	3860.941580	6.673523	-0.032247	3.392788
157.908237	3869.037499	6.678528	-0.032300	3.396164
158.014353	3876.947608	6.683533	-0.032326	3.399454
158.459022	3884.972581	6.688538	-0.032414	3.402801
158.553583	3892.976877	6.693542	-0.032437	3.406123
158.708182	3901.009680	6.698547	-0.032471	3.409456
159.163681	3909.057893	6.703552	-0.032562	3.412803
159.428794	3917.069561	6.708557	-0.032617	3.416124
159.786045	3925.085325	6.713562	-0.032689	3.419447
159.726902	3933.107814	6.718566	-0.032683	3.422756
159.762270	3941.178765	6.723571	-0.032695	3.426084
159.982831	3949.194611	6.728576	-0.032742	3.429393
160.252027	3957.240898	6.733581	-0.032797	3.432713
160.523253	3965.283544	6.738586	-0.032853	3.436027
160.615324	3973.265777	6.743590	-0.032876	3.439308
160.754268	3981.302885	6.748595	-0.032907	3.442610
161.250241	3989.314259	6.753600	-0.033005	3.445910
161.399264	3997.323475	6.758605	-0.033038	3.449194
161.681144	4005.383895	6.763610	-0.033096	3.452501
161.761654	4013.435527	6.768614	-0.033117	3.455794
162.161571	4021.398083	6.773619	-0.033197	3.459058
162.342742	4029.473944	6.778624	-0.033236	3.462358
162.571848	4037.454889	6.783629	-0.033284	3.465618
162.908634	4045.531552	6.788634	-0.033353	3.468917
162.980917	4053.587183	6.793638	-0.033371	3.472196
163.068303	4061.635435	6.798643	-0.033393	3.475469
163.328192	4069.627659	6.803648	-0.033447	3.478721
163.534698	4077.617072	6.808653	-0.033491	3.481968
163.887288	4085.639545	6.813658	-0.033562	3.485230
164.180112	4093.641991	6.818662	-0.033622	3.488479
164.569935	4101.681512	6.823667	-0.033700	3.491743
164.681794	4109.728823	6.828672	-0.033727	3.494998
164.929273	4117.711220	6.833677	-0.033778	3.498228
165.143640	4125.778817	6.838682	-0.033824	3.501488
165.176162	4133.757290	6.843686	-0.033835	3.504704
165.339991	4141.821410	6.848691	-0.033871	3.507955
165.691058	4149.860002	6.853696	-0.033942	3.511199
165.802099	4157.860155	6.858701	-0.033968	3.514417
166.168071	4165.914259	6.863706	-0.034042	3.517661
166.315020	4173.935899	6.868710	-0.034075	3.520883
166.372936	4181.904723	6.873715	-0.034091	3.524077
166.730419	4189.962535	6.878720	-0.034163	3.527314
166.813875	4197.984711	6.883725	-0.034184	3.530525
167.059647	4206.035542	6.888730	-0.034235	3.533749
167.201620	4214.071966	6.893734	-0.034267	3.536962
167.272828	4222.120323	6.898739	-0.034286	3.540174
167.642088	4230.114415	6.903744	-0.034360	3.543371
167.795439	4238.140734	6.908749	-0.034394	3.546571
168.114477	4246.172187	6.913754	-0.034459	3.549775
168.286871	4254.300596	6.918758	-0.034497	3.553010
168.503680	4262.314403	6.923763	-0.034543	3.556198
168.694883	4270.267331	6.928768	-0.034584	3.559359
168.820818	4278.248806	6.933773	-0.034613	3.562526
169.114189	4286.277929	6.938778	-0.034673	3.565714
169.500041	4294.284669	6.943782	-0.034750	3.568892
169.383972	4302.336403	6.948787	-0.034734	3.572072
169.755559	4310.384046	6.953792	-0.034809	3.575260
170.001860	4318.358752	6.958797	-0.034860	3.578414
170.292201	4326.422974	6.963802	-0.034920	3.581601
170.298396	4334.434287	6.968806	-0.034926	3.584757
170.630348	4342.440161	6.973811	-0.034994	3.587916
170.956710	4350.486228	6.978816	-0.035060	3.591089
170.833479	4358.469414	6.983821	-0.035043	3.594221
170.874873	4366.547953	6.988826	-0.035056	3.597393
171.271955	4374.530868	6.993830	-0.035135	3.600534
171.505187	4382.511934	6.998835	-0.035184	3.603667
171.702208	4390.584034	7.003840	-0.035226	3.606833
171.805172	4398.601328	7.008845	-0.035251	3.609971
171.909554	4406.647934	7.013850	-0.035276	3.613118
172.095814	4414.691817	7.018854	-0.035316	3.616263
172.302926	4422.654040	7.023859	-0.035360	3.619375
172.477155	4430.722505	7.028864	-0.035398	3.622524
172.603308	4438.716422	7.033869	-0.035427	3.625640
172.804345	4446.748972	7.038874	-0.035470	3.628770
173.139382	4454.786437	7.043878	-0.035538	3.631903
173.343980	4462.845709	7.048883	-0.035582	3.635039
173.670156	4470.851281	7.053888	-0.035648	3.638154
173.632091	4478.899546	7.058893	-0.035646	3.641273
173.895108	4486.877483	7.063898	-0.035701	3.644371
173.723438	4494.946314	7.068902	-0.035674	3.647489
174.144664	4502.940106	7.073907	-0.035758	3.650591
174.349157	4510.980784	7.078912	-0.035802	3.653703
174.555845	4519.008039	7.083917	-0.035846	3.656807
174.605863	4527.021291	7.088922	-0.035860	3.659899
174.778868	4535.031386	7.093926	-0.035898	3.662991
175.054441	4543.063297	7.098931	-0.035955	3.666091
175.152507	4551.095436	7.103936	-0.035979	3.669183
175.442686	4559.101169	7.108941	-0.036038	3.672268
175.762833	4567.156490	7.113946	-0.036103	3.675370
175.836066	4575.165279	7.118950	-0.036123	3.678445
175.941759	4583.185162	7.123955	-0.036148	3.681523
176.219677	4591.183242	7.128960	-0.036205	3.684594
176.215052	4599.187268	7.133965	-0.036210	3.687658
176.632512	4607.242747	7.138970	-0.036293	3.690749
176.874751	4615.277485	7.143974	-0.036343	3.693826
177.006561	4623.260849	7.148979	-0.036373	3.696877
177.402763	4631.300692	7.153984	-0.036453	3.699954
177.426384	4639.311107	7.158989	-0.036463	3.703008
177.714943	4647.371589	7.163994	-0.036522	3.706085
177.770980	4655.390801	7.168998	-0.036538	3.709138
177.885603	4663.467897	7.174003	-0.036565	3.712212
178.253884	4671.539492	7.179008	-0.036639	3.715287
178.336065	4679.469319	7.184013	-0.036660	3.718300
178.335565	4687.507270	7.189018	-0.036665	3.721348
178.580887	4695.439675	7.194022	-0.036716	3.724360
178.960213	4703.484726	7.199027	-0.036792	3.727416
178.912892	4711.538902	7.204032	-0.036789	3.730462
179.030118	4719.527259	7.209037	-0.036816	3.733485
179.569312	4727.536840	7.214042	-0.036922	3.736523
179.553278	4735.578216	7.219046	-0.036925	3.739558
179.681856	4743.620360	7.224051	-0.036954	3.742593
180.041511	4751.618996	7.229056	-0.037027	3.745616
180.020052	4759.657158	7.234061	-0.037028	3.748642
180.231654	4767.713888	7.239066	-0.037073	3.751678
180.467797	4775.727530	7.244070	-0.037122	3.754695
180.612812	4783.729246	7.249075	-0.037155	3.757704
180.947250	4791.780706	7.254080	-0.037223	3.760733
181.106142	4799.736314	7.259085	-0.037258	3.763720
181.401967	4807.816643	7.264090	-0.037318	3.766754
181.354203	4815.825312	7.269094	-0.037315	3.769751
181.676757	4823.840361	7.274099	-0.037380	3.772757
181.971842	4831.941328	7.279104	-0.037441	3.775792
182.143531	4839.893331	7.284109	-0.037478	3.778765
182.319917	4847.947646	7.289114	-0.037517	3.781775
182.557507	4855.933589	7.294118	-0.037566	3.784758
182.620036	4863.976659	7.299123	-0.037584	3.787756
182.813050	4872.059462	7.304128	-0.037625	3.790769
182.925516	4880.041908	7.309133	-0.037652	3.793741
183.295806	4888.085974	7.314138	-0.037726	3.796739
183.502832	4896.024272	7.319142	-0.037770	3.799692
183.476820	4904.079349	7.324147	-0.037771	3.802681
183.693291	4912.088627	7.329152	-0.037816	3.805655
183.851978	4920.095010	7.334157	-0.037851	3.808625
183.972657	4928.167299	7.339162	-0.037879	3.811617
184.227615	4936.164737	7.344166	-0.037932	3.814581
184.511690	4944.170207	7.349171	-0.037991	3.817546
184.580888	4952.231640	7.354176	-0.038009	3.820525
184.788002	4960.167070	7.359181	-0.038053	3.823458
185.039871	4968.242479	7.364186	-0.038106	3.826441
185.063762	4976.235621	7.369190	-0.038116	3.829387
185.112461	4984.303927	7.374195	-0.038130	3.832359
185.380120	4992.306679	7.379200	-0.038186	3.835309
185.814284	5000.290162	7.384205	-0.038272	3.838253
185.789817	5008.364475	7.389210	-0.038273	3.841219
185.725306	5016.318794	7.394214	-0.038266	3.844137
186.237495	5024.356711	7.399219	-0.038367	3.847096
186.208971	5032.396258	7.404224	-0.038367	3.850042
186.124657	5040.462115	7.409229	-0.038357	3.852994
186.588206	5048.478189	7.414234	-0.038449	3.855937
186.864428	5056.470786	7.419238	-0.038506	3.858865
186.944511	5064.506008	7.424243	-0.038526	3.861802
187.136276	5072.507910	7.429248	-0.038567	3.864728
187.210990	5080.565160	7.434253	-0.038587	3.867669
187.464479	5088.585444	7.439258	-0.038640	3.870597
187.551224	5096.809590	7.444262	-0.038661	3.873595
187.777842	5104.827516	7.449267	-0.038709	3.876518
187.815115	5112.739850	7.454272	-0.038721	3.879396
187.845435	5120.696268	7.459277	-0.038733	3.882288
188.061939	5128.695992	7.464282	-0.038778	3.885198
188.037074	5136.715523	7.469286	-0.038779	3.888108
188.032459	5144.739123	7.474291	-0.038784	3.891017
188.321915	5152.801464	7.479296	-0.038843	3.893944
188.430955	5160.801005	7.484301	-0.038869	3.896842
188.565597	5168.764641	7.489306	-0.038900	3.899726
188.770942	5176.801381	7.494310	-0.038943	3.902635
189.018849	5184.818655	7.499315	-0.038995	3.905536
189.323779	5192.827799	7.504320	-0.039057	3.908433
189.353977	5200.845098	7.509325	-0.039068	3.911326
189.406913	5208.926969	7.514330	-0.039084	3.914240
189.633106	5216.931436	7.519334	-0.039131	3.917127
189.729202	5224.905171	7.524339	-0.039155	3.919999
190.079850	5232.910055	7.529344	-0.039225	3.922884
190.142210	5240.919095	7.534349	-0.039243	3.925764
190.420999	5248.952687	7.539354	-0.039300	3.928654
190.496525	5257.002549	7.544358	-0.039320	3.931544
190.667367	5264.994371	7.549363	-0.039357	3.934412
191.008009	5273.047257	7.554368	-0.039426	3.937304
191.000555	5281.036301	7.559373	-0.039430	3.940164
191.277608	5289.060706	7.564378	-0.039487	3.943040
191.331855	5297.078503	7.569382	-0.039503	3.945908
191.594470	5305.096294	7.574387	-0.039557	3.948777
191.768858	5313.197840	7.579392	-0.039595	3.951672
191.890320	5321.195931	7.584397	-0.039623	3.954528
192.066721	5329.219973	7.589402	-0.039661	3.957391
192.173881	5337.202407	7.594406	-0.039687	3.960237
192.266192	5345.209775	7.599411	-0.039710	3.963089
192.550236	5353.227807	7.604416	-0.039768	3.965946
192.496259	5361.185308	7.609421	-0.039763	3.968773
192.632362	5369.278348	7.614426	-0.039794	3.971650
193.160559	5377.282188	7.619430	-0.039898	3.974500
193.172895	5385.324275	7.624435	-0.039906	3.977352
193.318099	5393.339469	7.629440	-0.039938	3.980196
193.289295	5401.331572	7.634445	-0.039938	3.983026
193.417734	5409.372324	7.639450	-0.039968	3.985874
193.636779	5417.409385	7.644454	-0.040014	3.988720
193.631245	5425.414947	7.649459	-0.040019	3.991549
193.953759	5433.486264	7.654464	-0.040084	3.994405
194.127067	5441.465912	7.659469	-0.040122	3.997223
194.337271	5449.484128	7.664474	-0.040167	4.000054
194.537382	5457.504148	7.669478	-0.040209	4.002884
194.714414	5465.505261	7.674483	-0.040248	4.005704
195.048529	5473.544067	7.679488	-0.040316	4.008538
195.255679	5481.585526	7.684493	-0.040360	4.011369
195.467823	5489.618318	7.689498	-0.040405	4.014196
195.522006	5497.650552	7.694502	-0.040420	4.017017
195.652621	5505.627227	7.699507	-0.040450	4.019818
196.143100	5513.673824	7.704512	-0.040547	4.022647
196.093405	5521.684051	7.709517	-0.040543	4.025453
196.165466	5529.709697	7.714522	-0.040562	4.028265
196.331971	5537.727954	7.719526	-0.040599	4.031073
196.801506	5545.800388	7.724531	-0.040691	4.033903
196.770129	5553.869005	7.729536	-0.040691	4.036721
196.862648	5561.745640	7.734541	-0.040714	4.039473
196.986563	5569.799091	7.739546	-0.040742	4.042285
197.292387	5577.814648	7.744550	-0.040805	4.045085
197.057814	5585.820229	7.749555	-0.040767	4.047871
197.330919	5593.876215	7.754560	-0.040823	4.050680
197.639772	5601.861023	7.759565	-0.040886	4.053463
197.827815	5609.893323	7.764570	-0.040926	4.056259
198.184036	5617.870337	7.769574	-0.040998	4.059036
198.227847	5625.905464	7.774579	-0.041012	4.061826
198.402971	5633.893936	7.779584	-0.041050	4.064601
198.481573	5641.936935	7.784589	-0.041070	4.067391
198.738132	5649.997168	7.789594	-0.041123	4.070188
198.973147	5658.022447	7.794598	-0.041173	4.072970
198.994272	5666.034882	7.799603	-0.041182	4.075743
199.323675	5674.024145	7.804608	-0.041249	4.078510
199.428338	5682.008988	7.809613	-0.041274	4.081271
199.508505	5689.993934	7.814618	-0.041294	4.084030
199.619837	5698.094397	7.819622	-0.041321	4.086827
199.616187	5706.081835	7.824627	-0.041325	4.089581
199.743738	5714.129329	7.829632	-0.041355	4.092356
199.898206	5722.106029	7.834637	-0.041389	4.095106
200.219553	5730.181501	7.839642	-0.041454	4.097889
200.337645	5738.206893	7.844646	-0.041482	4.100651
200.341911	5746.193059	7.849651	-0.041488	4.103396
200.674008	5754.251153	7.854656	-0.041555	4.106168
200.975101	5762.252325	7.859661	-0.041617	4.108918
201.070140	5770.329616	7.864666	-0.041640	4.111690
201.133339	5778.319756	7.869670	-0.041657	4.114429
201.377473	5786.359535	7.874675	-0.041708	4.117186
201.505171	5794.349848	7.879680	-0.041738	4.119923
201.458888	5802.354724	7.884685	-0.041734	4.122661
201.621625	5810.341670	7.889690	-0.041770	4.125393
201.827869	5818.346103	7.894694	-0.041814	4.128130
201.746388	5826.384737	7.899699	-0.041804	4.130874
202.195060	5834.459794	7.904704	-0.041894	4.133634
202.480323	5842.470312	7.909709	-0.041952	4.136369
202.410457	5850.454092	7.914714	-0.041945	4.139088
202.606563	5858.517990	7.919718	-0.041987	4.141836
202.938426	5866.463189	7.924723	-0.042054	4.144543
203.172939	5874.534730	7.929728	-0.042103	4.147291
203.109724	5882.511897	7.934733	-0.042097	4.150000
203.476578	5890.572125	7.939738	-0.042171	4.152742
203.663754	5898.612790	7.944742	-0.042211	4.155473
203.697677	5906.598738	7.949747	-0.042223	4.158181
204.015939	5914.605030	7.954752	-0.042288	4.160898
204.156049	5922.582205	7.959757	-0.042319	4.163602
204.315632	5930.647014	7.964762	-0.042354	4.166333
204.290650	5938.673561	7.969766	-0.042355	4.169048
204.502292	5946.685383	7.974771	-0.042400	4.171758
204.664037	5954.716194	7.979776	-0.042436	4.174473
204.688611	5962.708751	7.984781	-0.042446	4.177171
205.021506	5970.733354	7.989786	-0.042513	4.179882
205.261118	5978.762664	7.994790	-0.042563	4.182592
205.231310	5986.723571	7.999795	-0.042563	4.185273
205.464392	5994.792367	8.004800	-0.042612	4.187993
205.559091	6002.817136	8.009805	-0.042635	4.190694
205.700242	6010.938518	8.014810	-0.042667	4.193426
205.715736	6018.965172	8.019814	-0.042676	4.196124
205.885817	6026.837742	8.024819	-0.042713	4.198769
206.435893	6034.915579	8.029824	-0.042821	4.201486
206.457151	6042.837541	8.034829	-0.042830	4.204143
206.690331	6050.900513	8.039834	-0.042879	4.206848
206.686277	6058.928544	8.044838	-0.042884	4.209537
206.970843	6066.913685	8.049843	-0.042942	4.212213
207.221114	6074.996561	8.054848	-0.042994	4.214919
207.210045	6082.955329	8.059853	-0.042998	4.217580
207.422009	6090.964765	8.064858	-0.043043	4.220258
207.624880	6098.982462	8.069862	-0.043086	4.222937
207.755312	6106.970052	8.074867	-0.043116	4.225604
208.008449	6115.042485	8.079872	-0.043168	4.228298
207.868513	6123.052969	8.084877	-0.043148	4.230966
208.096287	6131.103712	8.089882	-0.043196	4.233649
208.371097	6139.121709	8.094886	-0.043252	4.236320
208.383998	6147.073534	8.099891	-0.043260	4.238965
208.535011	6155.146660	8.104896	-0.043294	4.241650
208.877718	6163.100147	8.109901	-0.043363	4.244296
208.995466	6171.156319	8.114906	-0.043391	4.246971
209.044754	6179.153647	8.119910	-0.043405	4.249625
208.995872	6187.219948	8.124915	-0.043402	4.252299
209.319637	6195.263146	8.129920	-0.043467	4.254967
209.227015	6203.258786	8.134925	-0.043456	4.257614
209.643252	6211.221965	8.139930	-0.043539	4.260253
209.892766	6219.274072	8.144934	-0.043591	4.262918
210.034209	6227.252015	8.149939	-0.043622	4.265556
209.986556	6235.363842	8.154944	-0.043619	4.268235
210.019222	6243.349972	8.159949	-0.043631	4.270872
210.479275	6251.421697	8.164954	-0.043722	4.273538
210.714773	6259.443868	8.169958	-0.043771	4.276185
210.636062	6267.394857	8.174963	-0.043762	4.278804
211.028553	6275.390799	8.179968	-0.043841	4.281441
211.046627	6283.384261	8.184973	-0.043849	4.284071
211.174088	6291.494798	8.189978	-0.043879	4.286740
211.503367	6299.497079	8.194982	-0.043945	4.289372
211.597408	6307.515009	8.199987	-0.043968	4.292007
211.705920	6315.567998	8.204992	-0.043994	4.294651
211.949079	6323.549413	8.209997	-0.044045	4.297271
212.158527	6331.544243	8.215002	-0.044089	4.299894
212.046757	6339.568922	8.220006	-0.044074	4.302522
212.176844	6347.580308	8.225011	-0.044104	4.305147
212.558022	6355.597387	8.230016	-0.044180	4.307773
212.613426	6363.621430	8.235021	-0.044196	4.310398
212.880196	6371.683699	8.240026	-0.044251	4.313035
212.879264	6379.710343	8.245030	-0.044257	4.315657
213.067928	6387.655269	8.250035	-0.044297	4.318252
213.190443	6395.704195	8.255040	-0.044326	4.320879
213.210668	6403.644479	8.260045	-0.044335	4.323468
213.404117	6411.726564	8.265050	-0.044376	4.326103
213.827287	6419.729953	8.270054	-0.044461	4.328712
213.917682	6427.741796	8.275059	-0.044483	4.331320
214.212187	6435.791530	8.280064	-0.044543	4.333941
214.165595	6443.787305	8.285069	-0.044540	4.336540
214.364381	6451.751875	8.290074	-0.044583	4.339128
214.754943	6459.849983	8.295078	-0.044661	4.341760
214.752968	6467.763108	8.300083	-0.044666	4.344328
214.804054	6475.883028	8.305088	-0.044681	4.346961
214.969204	6483.861976	8.310093	-0.044717	4.349548
215.041101	6491.956601	8.315098	-0.044736	4.352170
215.151983	6499.998437	8.320102	-0.044762	4.354774
215.175562	6507.990887	8.325107	-0.044772	4.357360
215.627066	6515.960332	8.330112	-0.044862	4.359939
215.733041	6523.922110	8.335117	-0.044887	4.362512
215.791267	6531.910840	8.340122	-0.044903	4.365092
216.023080	6539.997771	8.345126	-0.044952	4.367703
216.157306	6547.934633	8.350131	-0.044982	4.370264
216.523664	6556.009429	8.355136	-0.045056	4.372869
216.570929	6564.045684	8.360141	-0.045070	4.375458
216.742670	6572.065037	8.365146	-0.045108	4.378041
216.777868	6580.053833	8.370150	-0.045120	4.380612
216.970456	6588.037713	8.375155	-0.045161	4.383180
217.434216	6596.075952	8.380160	-0.045253	4.385766
217.427544	6604.110881	8.385165	-0.045257	4.388347
217.436378	6612.109415	8.390170	-0.045264	4.390914
217.435443	6620.204315	8.395174	-0.045270	4.393511
217.522862	6628.220690	8.400179	-0.045292	4.396082
217.933305	6636.222719	8.405184	-0.045373	4.398648
217.942294	6644.199213	8.410189	-0.045381	4.401202
217.981771	6652.177901	8.415194	-0.045393	4.403756
218.151089	6660.215761	8.420198	-0.045430	4.406328
218.403129	6668.219943	8.425203	-0.045483	4.408888
218.779110	6676.314895	8.430208	-0.045558	4.411476
218.850904	6684.289440	8.435213	-0.045577	4.414023
219.058950	6692.347747	8.440218	-0.045622	4.416595
219.159328	6700.329255	8.445222	-0.045646	4.419141
219.181826	6708.368515	8.450227	-0.045655	4.421704
219.498076	6716.343382	8.455232	-0.045720	4.424246
219.431259	6724.354099	8.460237	-0.045713	4.426796
219.723166	6732.412311	8.465242	-0.045773	4.429361
219.682154	6740.505612	8.470246	-0.045771	4.431935
219.812725	6748.491136	8.475251	-0.045800	4.434473
220.268005	6756.564284	8.480256	-0.045891	4.437040
220.239866	6764.482667	8.485261	-0.045891	4.439553
220.277038	6772.468633	8.490266	-0.045903	4.442087
220.548761	6780.477723	8.495270	-0.045959	4.444628
220.721980	6788.516457	8.500275	-0.045997	4.447176
221.060400	6796.541965	8.505280	-0.046066	4.449719
221.040965	6804.600445	8.510285	-0.046068	4.452270
221.344264	6812.585460	8.515290	-0.046129	4.454797
221.260391	6820.626342	8.520294	-0.046119	4.457339
221.404881	6828.572160	8.525299	-0.046152	4.459850
221.679462	6836.640619	8.530304	-0.046208	4.462399
221.859350	6844.600148	8.535309	-0.046247	4.464912
222.005953	6852.683425	8.540314	-0.046280	4.467463
221.862617	6860.654828	8.545318	-0.046259	4.469975
221.922201	6868.719582	8.550323	-0.046276	4.472516
222.210698	6876.756688	8.555328	-0.046335	4.475048
222.197569	6884.720360	8.560333	-0.046338	4.477555
222.369961	6892.703407	8.565338	-0.046375	4.480066
222.647867	6900.757463	8.570343	-0.046433	4.482599
222.726175	6908.749648	8.575347	-0.046453	4.485111
222.890664	6916.805158	8.580352	-0.046489	4.487641
223.002262	6924.807099	8.585357	-0.046515	4.490152
223.110900	6932.846456	8.590362	-0.046541	4.492674
223.275661	6940.868932	8.595367	-0.046577	4.495190
223.648525	6948.851193	8.600371	-0.046652	4.497692
223.656818	6956.877253	8.605376	-0.046659	4.500205
223.626585	6964.847282	8.610381	-0.046659	4.502699
223.811065	6972.864797	8.615386	-0.046699	4.505207
224.022555	6980.949570	8.620391	-0.046744	4.507735
223.986435	6988.925070	8.625395	-0.046742	4.510227
224.318697	6997.018016	8.630400	-0.046810	4.512755
224.554044	7005.053359	8.635405	-0.046859	4.515263
224.492948	7013.001431	8.640410	-0.046853	4.517742
224.468852	7020.969605	8.645415	-0.046854	4.520226
224.592042	7028.968149	8.650419	-0.046882	4.522718
224.943523	7036.974555	8.655424	-0.046953	4.525212
225.238360	7045.049135	8.660429	-0.047014	4.527725
225.226101	7053.025966	8.665434	-0.047017	4.530206
225.425538	7061.074107	8.670439	-0.047060	4.532709
225.703718	7069.064971	8.675443	-0.047117	4.535192
225.878442	7077.115272	8.680448	-0.047155	4.537692
226.031795	7085.103805	8.685453	-0.047189	4.540172
226.179076	7093.112917	8.690458	-0.047222	4.542656
226.314980	7101.079196	8.695463	-0.047253	4.545126
226.492849	7109.129270	8.700467	-0.047291	4.547620
226.584621	7117.174202	8.705472	-0.047314	4.550112
226.637812	7125.231850	8.710477	-0.047329	4.552606
226.845612	7133.278066	8.715482	-0.047374	4.555095
227.070034	7141.276171	8.720487	-0.047421	4.557568
227.162200	7149.186309	8.725491	-0.047443	4.560012
227.081593	7157.252132	8.730496	-0.047434	4.562503
227.392780	7165.228705	8.735501	-0.047497	4.564965
227.612041	7173.256632	8.740506	-0.047544	4.567442
227.759846	7181.325731	8.745511	-0.047577	4.569930
227.884660	7189.324376	8.750515	-0.047605	4.572394
228.335855	7197.404428	8.755520	-0.047695	4.574883
228.356489	7205.340204	8.760525	-0.047704	4.577326
228.373389	7213.332015	8.765530	-0.047713	4.579784
228.660835	7221.407666	8.770535	-0.047772	4.582268
228.597314	7229.337251	8.775539	-0.047766	4.584704
228.698833	7237.449621	8.780544	-0.047790	4.587196
229.178858	7245.436481	8.785549	-0.047885	4.589648
229.085991	7253.524540	8.790554	-0.047873	4.592129
229.183587	7261.574878	8.795559	-0.047897	4.594598
229.228919	7269.512486	8.800563	-0.047911	4.597031
229.687399	7277.487451	8.805568	-0.048002	4.599474
229.529895	7285.539918	8.810573	-0.047978	4.601939
229.650220	7293.525988	8.815578	-0.048006	4.604382
230.018112	7301.604010	8.820583	-0.048080	4.606853
230.188500	7309.538465	8.825587	-0.048117	4.609278
230.074909	7317.641835	8.830592	-0.048101	4.611753
230.332208	7325.610391	8.835597	-0.048155	4.614186
230.588420	7333.672292	8.840602	-0.048208	4.616647
230.544580	7341.622809	8.845607	-0.048205	4.619071
230.475026	7349.652267	8.850611	-0.048198	4.621519
230.792102	7357.615506	8.855616	-0.048262	4.623945
230.913178	7365.686464	8.860621	-0.048290	4.626403
230.928300	7373.684698	8.865626	-0.048299	4.628837
231.240575	7381.792253	8.870631	-0.048362	4.631303
231.293007	7389.767261	8.875635	-0.048377	4.633728
231.417418	7397.760983	8.880640	-0.048406	4.636157
231.437026	7405.705290	8.885645	-0.048415	4.638569
231.873290	7413.792463	8.890650	-0.048502	4.641024
231.887134	7421.819325	8.895655	-0.048510	4.643459
231.849767	7429.761720	8.900659	-0.048509	4.645867
232.031263	7437.793301	8.905664	-0.048548	4.648301
231.993888	7445.842984	8.910669	-0.048546	4.650739
232.164342	7453.870696	8.915674	-0.048584	4.653170
232.339161	7461.938815	8.920679	-0.048622	4.655611
232.380535	7469.892040	8.925683	-0.048635	4.658016
232.506346	7477.919957	8.930688	-0.048664	4.660442
232.671862	7485.884044	8.935693	-0.048700	4.662848
233.135480	7493.880398	8.940698	-0.048792	4.665262
233.206282	7501.966354	8.945703	-0.048811	4.667702
233.032007	7509.937476	8.950707	-0.048784	4.670107
233.291192	7518.108338	8.955712	-0.048837	4.672570
233.414548	7526.119221	8.960717	-0.048866	4.674983
233.410930	7534.029974	8.965722	-0.048871	4.677366
233.621385	7542.028871	8.970727	-0.048915	4.679773
233.780561	7550.000561	8.975731	-0.048950	4.682171
233.842055	7558.036099	8.980736	-0.048967	4.684587
233.942768	7566.041755	8.985741	-0.048992	4.686993
234.075883	7574.041367	8.990746	-0.049022	4.689396
234.375667	7582.147061	8.995751	-0.049083	4.691829
234.516114	7590.155129	9.000755	-0.049115	4.694231
235.062277	7598.146065	9.005760	-0.049222	4.696627
235.161542	7606.131000	9.010765	-0.049246	4.699020
234.903834	7614.144682	9.015770	-0.049204	4.701422
235.176489	7622.179701	9.020775	-0.049260	4.703827
235.458061	7630.129281	9.025779	-0.049318	4.706206
235.597427	7638.139348	9.030784	-0.049349	4.708602
235.646578	7646.251041	9.035789	-0.049364	4.711027
235.745138	7654.242976	9.040794	-0.049388	4.713415
235.980244	7662.279846	9.045799	-0.049437	4.715815
235.795095	7670.266170	9.050803	-0.049408	4.718199
236.072706	7678.307492	9.055808	-0.049465	4.720598
236.060335	7686.293958	9.060813	-0.049468	4.722980
236.299942	7694.309743	9.065818	-0.049518	4.725368
236.394445	7702.375539	9.070823	-0.049542	4.727771
236.438667	7710.316022	9.075827	-0.049555	4.730135
236.800787	7718.418800	9.080832	-0.049628	4.732546
236.839098	7726.378909	9.085837	-0.049641	4.734914
236.936107	7734.417127	9.090842	-0.049664	4.737303
237.340084	7742.409987	9.095847	-0.049745	4.739677
237.305434	7750.444585	9.100851	-0.049744	4.742064
237.607156	7758.438345	9.105856	-0.049806	4.744436
237.713310	7766.476251	9.110861	-0.049831	4.746820
237.601218	7774.450601	9.115866	-0.049816	4.749186
237.882435	7782.554378	9.120871	-0.049874	4.751587
237.897189	7790.545546	9.125875	-0.049882	4.753954
238.226336	7798.578043	9.130880	-0.049949	4.756332
238.179228	7806.541747	9.135885	-0.049945	4.758689
238.356965	7814.539488	9.140890	-0.049984	4.761054
238.740665	7822.607122	9.145895	-0.050061	4.763438
238.591084	7830.513951	9.150899	-0.050038	4.765775
238.784249	7838.580037	9.155904	-0.050080	4.768157
239.076404	7846.604942	9.160909	-0.050140	4.770525
239.276938	7854.646543	9.165914	-0.050183	4.772897
239.330891	7862.680801	9.170919	-0.050198	4.775266
239.361119	7870.734657	9.175923	-0.050209	4.777640
239.557843	7878.719508	9.180928	-0.050251	4.779992
239.676137	7886.694588	9.185933	-0.050279	4.782340
239.894468	7894.673955	9.190938	-0.050325	4.784688
239.823642	7902.744591	9.195943	-0.050317	4.787062
239.878018	7910.695667	9.200947	-0.050333	4.789400
239.974660	7918.741578	9.205952	-0.050356	4.791764
240.192352	7926.806021	9.210957	-0.050403	4.794132
240.291671	7934.783462	9.215962	-0.050427	4.796474
240.280798	7942.753628	9.220967	-0.050430	4.798813
240.363720	7950.797239	9.225971	-0.050451	4.801172
240.586736	7958.770298	9.230976	-0.050498	4.803509
240.735871	7966.803734	9.235981	-0.050531	4.805862
240.905156	7974.828695	9.240986	-0.050568	4.808212
241.151782	7982.867416	9.245991	-0.050620	4.810564
241.279105	7990.231626	9.250995	-0.050648	4.812718
241.300732	7994.732015	9.256000	-0.050656	4.814034

241.554420	7997.235394	9.261005	-0.050705	4.814765
241.659870	7998.483165	9.266010	-0.050725	4.815129
241.690183	7998.974861	9.271015	-0.050732	4.815273
241.497796	7999.919983	9.276019	-0.050697	4.815550
241.830763	7999.959603	9.281024	-0.050759	4.815560
241.952535	7999.934915	9.286029	-0.050782	4.815552
241.865290	7999.927109	9.291034	-0.050766	4.815551
241.961647	7999.940449	9.296039	-0.050784	4.815554
241.892545	7999.898768	9.301043	-0.050772	4.815542
241.861750	7999.952751	9.306048	-0.050766	4.815558
242.155687	7999.938343	9.311053	-0.050821	4.815552
242.201368	7999.939111	9.316058	-0.050830	4.815552
242.155728	7999.945866	9.321063	-0.050822	4.815555
241.890366	7999.906326	9.326067	-0.050773	4.815544
242.274338	7999.909403	9.331072	-0.050844	4.815543
242.213080	7999.916971	9.336077	-0.050833	4.815546
242.061230	7999.931606	9.341082	-0.050805	4.815551
242.376825	7999.949587	9.346087	-0.050864	4.815555
242.449788	7999.895270	9.351091	-0.050878	4.815538
242.417174	7999.937478	9.356096	-0.050872	4.815551
242.423298	7999.922651	9.361101	-0.050874	4.815547
242.438165	7999.932527	9.366106	-0.050877	4.815549
242.280510	7999.928914	9.371111	-0.050848	4.815549
242.321681	7999.915726	9.376115	-0.050856	4.815545
242.452267	7999.970204	9.381120	-0.050880	4.815560
242.641473	7999.945547	9.386125	-0.050916	4.815552
242.657038	7999.890294	9.391130	-0.050919	4.815536
242.716769	7999.911581	9.396135	-0.050930	4.815542
242.431925	7999.914437	9.401139	-0.050877	4.815544
242.591225	7999.953365	9.406144	-0.050907	4.815555
242.619437	7999.915404	9.411149	-0.050913	4.815543
242.769961	7999.909339	9.416154	-0.050941	4.815541
242.701458	7999.958436	9.421159	-0.050929	4.815556
242.640574	7999.904073	9.426163	-0.050918	4.815540
242.798693	7999.951525	9.431168	-0.050947	4.815553
242.705822	7999.919066	9.436173	-0.050930	4.815544
242.614030	7999.930408	9.441178	-0.050914	4.815548
242.961937	7999.945714	9.446183	-0.050979	4.815551
242.881428	7999.951901	9.451187	-0.050964	4.815553
242.992100	7999.962272	9.456192	-0.050985	4.815555
242.954625	7999.956345	9.461197	-0.050978	4.815554
242.810981	7999.946551	9.466202	-0.050952	4.815552
243.030359	7999.954423	9.471207	-0.050993	4.815553
242.922021	7999.917440	9.476211	-0.050973	4.815542
243.180024	7999.937688	9.481216	-0.051021	4.815547
242.822637	7999.955379	9.486221	-0.050955	4.815554
243.030870	7999.943847	9.491226	-0.050994	4.815550
243.229230	7999.983413	9.496231	-0.051031	4.815560
243.010027	7999.974523	9.501235	-0.050991	4.815559
242.939713	7999.964857	9.506240	-0.050978	4.815556
242.998799	7999.945554	9.511245	-0.050989	4.815550
243.050311	7999.942146	9.516250	-0.050999	4.815549
243.256695	7999.979707	9.521255	-0.051038	4.815559
243.171467	7999.912131	9.526259	-0.051022	4.815540
243.269605	7999.940452	9.531264	-0.051040	4.815547
243.344919	7999.948112	9.536269	-0.051055	4.815549
243.185980	7999.959426	9.541274	-0.051025	4.815553
243.241747	7999.982785	9.546279	-0.051036	4.815560
242.957674	7999.960023	9.551283	-0.050983	4.815555
243.112933	7999.971121	9.556288	-0.051013	4.815557
243.133963	7999.941586	9.561293	-0.051017	4.815548
243.218236	7999.964342	9.566298	-0.051033	4.815555
243.242368	7999.976506	9.571303	-0.051038	4.815558
243.051795	7999.946725	9.576307	-0.051002	4.815550
243.263055	7999.968347	9.581312	-0.051042	4.815556
243.333972	7999.974867	9.586317	-0.051055	4.815557
243.370155	7999.964801	9.591322	-0.051062	4.815554
243.376567	7999.994831	9.596327	-0.051064	4.815563
243.328415	7999.970575	9.601331	-0.051055	4.815556
243.417452	7999.994477	9.606336	-0.051072	4.815562
243.323051	7999.957720	9.611341	-0.051055	4.815552
243.397099	7999.945068	9.616346	-0.051069	4.815548
243.391394	8000.001598	9.621351	-0.051068	4.815565
243.451573	7999.924646	9.626355	-0.051079	4.815542
243.557724	7999.991543	9.631360	-0.051100	4.815561
243.489015	7999.957341	9.636365	-0.051087	4.815551
243.374259	7999.957629	9.641370	-0.051066	4.815552
243.603041	7999.965655	9.646375	-0.051109	4.815553
243.581595	7999.938631	9.651379	-0.051105	4.815545
243.565265	7999.999259	9.656384	-0.051102	4.815563
243.522797	7999.930244	9.661389	-0.051095	4.815543
243.471774	7999.902738	9.666394	-0.051085	4.815535
243.795198	7999.989197	9.671399	-0.051146	4.815559
243.512274	7999.960044	9.676403	-0.051093	4.815552
243.448576	7999.938739	9.681408	-0.051082	4.815546
243.518912	7999.968743	9.686413	-0.051095	4.815554
243.515863	7999.962310	9.691418	-0.051095	4.815552
243.546044	7999.983116	9.696423	-0.051101	4.815558
243.710464	7999.944172	9.701427	-0.051132	4.815546
243.691109	7999.963102	9.706432	-0.051128	4.815552
243.604646	7999.963852	9.711437	-0.051113	4.815552
243.783486	7999.966792	9.716442	-0.051146	4.815552
243.668117	7999.977749	9.721447	-0.051125	4.815556
243.438117	7999.947324	9.726451	-0.051082	4.815548
243.764468	7999.983639	9.731456	-0.051143	4.815557
243.784162	7999.976509	9.736461	-0.051147	4.815555
243.635691	7999.961296	9.741466	-0.051120	4.815552
243.700282	7999.955965	9.746471	-0.051132	4.815550
243.636086	7999.949602	9.751475	-0.051121	4.815548
243.788228	8000.005503	9.756480	-0.051149	4.815564
243.620102	7999.992106	9.761485	-0.051118	4.815561
243.817590	7999.996418	9.766490	-0.051155	4.815561
243.868649	8000.017565	9.771495	-0.051165	4.815567
243.736708	7999.942818	9.776499	-0.051141	4.815546
243.811168	7999.909883	9.781504	-0.051155	4.815536
243.961570	7999.968959	9.786509	-0.051183	4.815552
243.944468	7999.987926	9.791514	-0.051180	4.815558
243.992380	8000.002615	9.796519	-0.051189	4.815562
243.888735	7999.979589	9.801523	-0.051170	4.815556
243.965804	8000.002228	9.806528	-0.051185	4.815562
243.900284	7999.992640	9.811533	-0.051173	4.815559
243.950545	7999.972125	9.816538	-0.051183	4.815553
243.958657	8000.025677	9.821543	-0.051184	4.815569
244.028738	7999.986262	9.826547	-0.051198	4.815557
244.063623	8000.010349	9.831552	-0.051205	4.815564
243.998491	7999.979409	9.836557	-0.051193	4.815555
243.945605	7999.982841	9.841562	-0.051183	4.815556
244.002330	7999.986994	9.846567	-0.051194	4.815557
243.782690	7999.975960	9.851571	-0.051153	4.815555
243.987247	8000.011357	9.856576	-0.051192	4.815564
243.835083	7999.981133	9.861581	-0.051164	4.815556
243.736378	7999.953917	9.866586	-0.051145	4.815549
243.949786	7999.998002	9.871591	-0.051185	4.815561
243.825891	7999.937269	9.876595	-0.051163	4.815543
243.778379	7999.969623	9.881600	-0.051154	4.815553
243.779118	7999.973931	9.886605	-0.051154	4.815554
243.898338	7999.997257	9.891610	-0.051177	4.815561
244.056329	8000.013741	9.896615	-0.051207	4.815565
243.908089	7999.954747	9.901619	-0.051179	4.815548
243.855349	7999.983812	9.906624	-0.051170	4.815557
243.808608	7999.975598	9.911629	-0.051161	4.815555
243.855026	7999.982786	9.916634	-0.051170	4.815557
243.784551	8000.004086	9.921639	-0.051157	4.815563
243.907535	7999.992233	9.926643	-0.051181	4.815559
243.863889	8000.012903	9.931648	-0.051173	4.815565
243.921467	7999.982896	9.936653	-0.051184	4.815556
243.979438	7999.967846	9.941658	-0.051195	4.815552
244.027934	8000.017786	9.946663	-0.051204	4.815566
243.799435	7999.962822	9.951667	-0.051162	4.815551
243.919785	8000.015001	9.956672	-0.051184	4.815566
244.061099	7999.915876	9.961677	-0.051211	4.815536
243.760709	7999.906729	9.966682	-0.051155	4.815535
244.032368	7999.932542	9.971687	-0.051206	4.815541
244.015570	7999.917340	9.976691	-0.051203	4.815537
244.033797	7999.969990	9.981696	-0.051207	4.815552
243.976180	7999.985092	9.986701	-0.051197	4.815557
244.075101	7999.977118	9.991706	-0.051215	4.815554
244.235644	7999.997916	9.996711	-0.051245	4.815559
244.123650	7999.972618	10.001715	-0.051225	4.815552
244.196786	8000.003736	10.006720	-0.051239	4.815561
244.484432	7999.997774	10.011725	-0.051293	4.815558
244.317788	7999.987603	10.016730	-0.051262	4.815556
244.475165	8000.022232	10.021735	-0.051291	4.815565
244.442121	7999.992882	10.026739	-0.051285	4.815557
244.407879	7999.991279	10.031744	-0.051279	4.815556
244.837183	7999.991900	10.036749	-0.051360	4.815554
244.678612	7999.980793	10.041754	-0.051330	4.815552
244.657188	8000.007165	10.046759	-0.051327	4.815560
244.489915	7999.989508	10.051763	-0.051296	4.815555
244.577564	8000.035816	10.056768	-0.051312	4.815568
244.630767	8000.020688	10.061773	-0.051323	4.815564
244.462907	8000.006226	10.066778	-0.051292	4.815560
244.592713	8000.028658	10.071783	-0.051316	4.815566
244.456240	7999.991213	10.076787	-0.051291	4.815556
244.460875	7999.997720	10.081792	-0.051292	4.815558
244.361070	8000.000387	10.086797	-0.051274	4.815559
244.475552	8000.000142	10.091802	-0.051295	4.815558
244.632367	8000.030491	10.096807	-0.051325	4.815567
244.653955	7999.991353	10.101811	-0.051329	4.815555
244.686624	8000.012201	10.106816	-0.051335	4.815561
244.553680	8000.021802	10.111821	-0.051311	4.815564
244.696974	7999.993194	10.116826	-0.051338	4.815555
244.797429	8000.010876	10.121831	-0.051357	4.815560
244.689328	7999.958942	10.126835	-0.051337	4.815545
244.561316	7999.996391	10.131840	-0.051313	4.815557
244.674735	8000.007877	10.136845	-0.051335	4.815560
244.643379	8000.012728	10.141850	-0.051329	4.815561
244.457626	8000.012925	10.146855	-0.051295	4.815562
244.405664	7999.969383	10.151859	-0.051285	4.815550
244.547709	8000.013374	10.156864	-0.051312	4.815562
244.792482	8000.033411	10.161869	-0.051358	4.815567
244.457725	8000.007681	10.166874	-0.051296	4.815561
244.525569	8000.016287	10.171879	-0.051309	4.815563
244.630979	7999.988128	10.176883	-0.051329	4.815554
244.614248	7999.976132	10.181888	-0.051326	4.815551
244.730055	7999.994064	10.186893	-0.051348	4.815555
244.587762	8000.002445	10.191898	-0.051321	4.815558
244.691241	8000.031924	10.196903	-0.051341	4.815567
244.611773	7999.995409	10.201907	-0.051326	4.815556
244.636571	8000.011856	10.206912	-0.051331	4.815561
244.683225	7999.981671	10.211917	-0.051340	4.815552
244.365560	7999.967968	10.216922	-0.051281	4.815549
244.450267	8000.016363	10.221927	-0.051298	4.815563
244.318633	7999.981133	10.226931	-0.051273	4.815553
244.530070	8000.019848	10.231936	-0.051313	4.815564
244.464983	7999.998519	10.236941	-0.051301	4.815558
244.655301	8000.008055	10.241946	-0.051337	4.815560
244.546739	8000.012715	10.246951	-0.051317	4.815562
244.506397	8000.002469	10.251955	-0.051310	4.815559
244.494554	8000.023658	10.256960	-0.051308	4.815565
244.591805	8000.013521	10.261965	-0.051326	4.815562
244.516199	8000.018719	10.266970	-0.051312	4.815563
244.613256	8000.019258	10.271975	-0.051331	4.815563
244.639563	8000.009032	10.276979	-0.051336	4.815560
244.721800	8000.022145	10.281984	-0.051351	4.815563
244.743836	8000.011848	10.286989	-0.051356	4.815560
244.471903	7999.993551	10.291994	-0.051305	4.815556
244.573534	8000.049699	10.296999	-0.051325	4.815572
244.407338	8000.001089	10.302003	-0.051294	4.815559
244.562365	8000.033544	10.307008	-0.051323	4.815567
244.667528	8000.023537	10.312013	-0.051343	4.815564
244.713015	7999.990128	10.317018	-0.051352	4.815554
244.810315	8000.048341	10.322023	-0.051370	4.815571
244.715297	8000.038270	10.327027	-0.051353	4.815568
244.810019	8000.032364	10.332032	-0.051370	4.815566
244.738727	8000.024816	10.337037	-0.051357	4.815564
244.818610	8000.006921	10.342042	-0.051373	4.815558
244.739703	8000.034491	10.347047	-0.051358	4.815567
244.739337	7999.972568	10.352051	-0.051358	4.815549
244.854564	7999.999034	10.357056	-0.051380	4.815556
244.976654	8000.003186	10.362061	-0.051403	4.815557
244.899887	7999.995550	10.367066	-0.051389	4.815555
244.952099	8000.024192	10.372071	-0.051399	4.815563
244.788430	8000.002322	10.377075	-0.051369	4.815557
244.688599	8000.027415	10.382080	-0.051351	4.815565
244.723195	8000.014120	10.387085	-0.051357	4.815561
244.773801	8000.000018	10.392090	-0.051367	4.815557
244.953326	8000.061709	10.397095	-0.051401	4.815574
244.800783	8000.027204	10.402099	-0.051372	4.815564
244.706113	8000.022479	10.407104	-0.051355	4.815563
244.987614	8000.020689	10.412109	-0.051408	4.815562
244.862728	8000.003723	10.417114	-0.051385	4.815557
244.937739	8000.045553	10.422119	-0.051399	4.815569
244.725392	8000.009005	10.427123	-0.051360	4.815559
244.779524	8000.050494	10.432128	-0.051370	4.815571
244.797549	8000.056151	10.437133	-0.051374	4.815573
244.815876	8000.012688	10.442138	-0.051377	4.815560
244.943071	8000.032943	10.447143	-0.051401	4.815565
244.747842	7999.978518	10.452147	-0.051365	4.815550
244.579899	7999.965122	10.457152	-0.051334	4.815547
244.804842	8000.007263	10.462157	-0.051376	4.815558
244.819832	8000.011803	10.467162	-0.051380	4.815560
244.646380	8000.037830	10.472167	-0.051348	4.815568
244.912096	7999.995200	10.477171	-0.051397	4.815554
245.085405	8000.029023	10.482176	-0.051430	4.815563
244.823090	8000.024766	10.487181	-0.051381	4.815563
244.675595	8000.014907	10.492186	-0.051354	4.815561
244.849061	8000.048732	10.497191	-0.051387	4.815570
244.873747	7999.992557	10.502195	-0.051391	4.815554
244.981440	8000.068027	10.507200	-0.051412	4.815575
244.961416	8000.031413	10.512205	-0.051408	4.815565
244.874021	8000.013991	10.517210	-0.051392	4.815560
244.868143	8000.029938	10.522215	-0.051391	4.815565
244.817637	8000.004574	10.527219	-0.051382	4.815557
244.771334	8000.020930	10.532224	-0.051374	4.815562
244.652738	8000.017950	10.537229	-0.051352	4.815562
244.753567	8000.018551	10.542234	-0.051371	4.815562
245.108282	8000.049995	10.547239	-0.051438	4.815569
244.752410	8000.023919	10.552243	-0.051372	4.815563
244.777340	8000.025418	10.557248	-0.051376	4.815564
245.136447	8000.044118	10.562253	-0.051444	4.815567
244.872860	7999.984305	10.567258	-0.051395	4.815551
244.966785	8000.018968	10.572263	-0.051413	4.815561
245.000707	7999.988575	10.577267	-0.051419	4.815552
245.033312	8000.027577	10.582272	-0.051425	4.815563
245.120444	8000.019411	10.587277	-0.051442	4.815560
244.738230	8000.042032	10.592282	-0.051371	4.815569
245.023639	8000.076616	10.597287	-0.051425	4.815577
245.174908	8000.037459	10.602291	-0.051453	4.815565
245.164079	8000.068276	10.607296	-0.051451	4.815574
244.990171	8000.030219	10.612301	-0.051419	4.815564
244.926102	8000.009973	10.617306	-0.051407	4.815558
245.082158	8000.040311	10.622311	-0.051437	4.815567
244.961280	8000.008459	10.627315	-0.051414	4.815558
244.875348	8000.044459	10.632320	-0.051399	4.815569
244.788578	8000.035590	10.637325	-0.051383	4.815567
245.008367	8000.015706	10.642330	-0.051424	4.815560
245.028245	8000.045957	10.647335	-0.051428	4.815568
244.942897	8000.005073	10.652339	-0.051412	4.815557
244.981217	8000.020673	10.657344	-0.051420	4.815561
244.949801	8000.005233	10.662349	-0.051414	4.815557
245.087672	8000.013914	10.667354	-0.051440	4.815559
245.091042	8000.044964	10.672359	-0.051441	4.815568
244.938058	8000.016860	10.677363	-0.051413	4.815560
245.026125	7999.995893	10.682368	-0.051430	4.815554
245.145704	7999.991461	10.687373	-0.051452	4.815552
244.951512	7999.977636	10.692378	-0.051416	4.815549
244.891964	8000.012998	10.697383	-0.051405	4.815559
244.993961	7999.986919	10.702387	-0.051425	4.815551
244.930499	7999.980567	10.707392	-0.051413	4.815550
244.880161	8000.011808	10.712397	-0.051404	4.815559
245.158912	7999.972595	10.717402	-0.051456	4.815546
245.167012	8000.021877	10.722407	-0.051458	4.815561
244.835425	7999.981246	10.727411	-0.051396	4.815550
245.049713	8000.006126	10.732416	-0.051437	4.815557
245.034483	8000.006969	10.737421	-0.051434	4.815557
245.059640	7999.965753	10.742426	-0.051439	4.815545
245.140362	8000.022628	10.747431	-0.051454	4.815561
245.151957	7999.986530	10.752435	-0.051457	4.815550
245.201927	8000.034360	10.757440	-0.051466	4.815564
245.326274	8000.037481	10.762445	-0.051490	4.815564
245.433540	8000.025372	10.767450	-0.051510	4.815560
245.438751	8000.039364	10.772455	-0.051511	4.815564
245.137110	7999.983202	10.777459	-0.051455	4.815549
245.006921	7999.991780	10.782464	-0.051431	4.815552
245.086370	8000.008052	10.787469	-0.051446	4.815557
244.961963	8000.018861	10.792474	-0.051424	4.815561
244.929181	8000.041845	10.797479	-0.051418	4.815567
245.098253	8000.043560	10.802483	-0.051449	4.815567
245.071975	8000.034611	10.807488	-0.051445	4.815565
245.213907	8000.050835	10.812493	-0.051472	4.815569
245.260502	8000.037735	10.817498	-0.051480	4.815565
245.257869	8000.069755	10.822503	-0.051480	4.815574
245.157536	8000.021150	10.827507	-0.051462	4.815560
245.384911	8000.041973	10.832512	-0.051504	4.815565
245.295031	8000.030918	10.837517	-0.051488	4.815562
244.989585	8000.021684	10.842522	-0.051431	4.815561
245.253201	8000.062321	10.847527	-0.051481	4.815572
245.206179	8000.029538	10.852531	-0.051472	4.815562
245.378807	8000.025972	10.857536	-0.051505	4.815561
245.100650	8000.034271	10.862541	-0.051453	4.815564
245.260647	8000.031566	10.867546	-0.051483	4.815563
245.410202	8000.062866	10.872551	-0.051511	4.815571
245.210116	8000.033992	10.877555	-0.051474	4.815564
245.144086	8000.027598	10.882560	-0.051462	4.815562
245.323169	8000.050837	10.887565	-0.051496	4.815568
245.002577	8000.019996	10.892570	-0.051436	4.815561
245.143522	8000.041544	10.897575	-0.051463	4.815566
245.122427	8000.018796	10.902579	-0.051459	4.815560
245.101344	8000.037698	10.907584	-0.051456	4.815565
245.121135	8000.002802	10.912589	-0.051460	4.815555
245.211998	8000.006445	10.917594	-0.051477	4.815556
245.508054	8000.052952	10.922599	-0.051532	4.815568
245.400192	8000.037331	10.927603	-0.051512	4.815564
245.164680	8000.024967	10.932608	-0.051469	4.815561
245.240087	8000.028357	10.937613	-0.051483	4.815562
245.271637	8000.024624	10.942618	-0.051489	4.815561
245.314276	8000.048839	10.947623	-0.051497	4.815567
245.237367	8000.029452	10.952627	-0.051483	4.815562
245.186292	8000.039321	10.957632	-0.051474	4.815565
245.308823	8000.007170	10.962637	-0.051497	4.815555
245.325067	8000.020274	10.967642	-0.051501	4.815559
245.409942	8000.057995	10.972647	-0.051517	4.815570
245.233003	8000.040178	10.977651	-0.051484	4.815565
245.119463	8000.044756	10.982656	-0.051463	4.815567
245.420178	8000.069980	10.987661	-0.051519	4.815573
245.254878	8000.042742	10.992666	-0.051489	4.815566
245.170278	8000.064880	10.997671	-0.051473	4.815573
245.185489	8000.028841	11.002675	-0.051476	4.815562
245.249526	8000.024570	11.007680	-0.051489	4.815561
245.357451	8000.033831	11.012685	-0.051509	4.815563
245.110959	8000.037307	11.017690	-0.051463	4.815565
245.344244	8000.068906	11.022695	-0.051507	4.815573
245.418805	8000.037040	11.027699	-0.051521	4.815563
245.464217	8000.039941	11.032704	-0.051530	4.815564
245.355453	8000.049936	11.037709	-0.051510	4.815567
245.232085	8000.003091	11.042714	-0.051487	4.815554
245.410218	8000.043402	11.047719	-0.051521	4.815565
245.409209	8000.023117	11.052723	-0.051521	4.815559
245.354178	8000.077777	11.057728	-0.051511	4.815576
245.352859	8000.063896	11.062733	-0.051511	4.815572
245.292300	8000.028756	11.067738	-0.051500	4.815562
245.589782	8000.072083	11.072743	-0.051556	4.815573
245.256836	8000.022884	11.077747	-0.051494	4.815560
245.333411	8000.022022	11.082752	-0.051508	4.815559
245.538380	8000.037139	11.087757	-0.051547	4.815563
245.419721	8000.007458	11.092762	-0.051525	4.815555
245.541153	8000.050047	11.097767	-0.051548	4.815567
245.334573	8000.042427	11.102771	-0.051510	4.815565
245.285182	8000.057664	11.107776	-0.051501	4.815570
245.317821	8000.049676	11.112781	-0.051507	4.815567
245.148243	8000.002077	11.117786	-0.051476	4.815554
245.396531	8000.051008	11.122791	-0.051522	4.815567
245.276053	8000.024502	11.127795	-0.051500	4.815560
245.208582	8000.025560	11.132800	-0.051488	4.815561
245.384043	8000.020972	11.137805	-0.051521	4.815559
245.172819	8000.007936	11.142810	-0.051482	4.815556
245.281429	8000.038568	11.147815	-0.051502	4.815564
245.618613	8000.025940	11.152819	-0.051565	4.815559
245.563646	8000.025067	11.157824	-0.051555	4.815559
245.640910	8000.074411	11.162829	-0.051570	4.815573
245.560367	8000.037876	11.167834	-0.051555	4.815563
245.722355	8000.065108	11.172839	-0.051586	4.815570
245.378122	8000.022132	11.177843	-0.051522	4.815559
245.486137	8000.028191	11.182848	-0.051542	4.815560
245.644865	8000.058574	11.187853	-0.051572	4.815568
245.424776	8000.026169	11.192858	-0.051531	4.815560
245.508349	8000.061732	11.197863	-0.051547	4.815570
245.310815	8000.014744	11.202867	-0.051511	4.815557
245.383984	8000.021302	11.207872	-0.051524	4.815559
245.461289	8000.066374	11.212877	-0.051539	4.815572
245.402283	8000.036599	11.217882	-0.051528	4.815563
245.550578	8000.061472	11.222887	-0.051556	4.815570
245.500607	8000.055340	11.227891	-0.051547	4.815568
245.310996	8000.057607	11.232896	-0.051512	4.815570
245.398502	8000.054788	11.237901	-0.051529	4.815568
245.311238	8000.029891	11.242906	-0.051513	4.815562
245.620459	8000.049915	11.247911	-0.051571	4.815566
245.527174	8000.038804	11.252915	-0.051554	4.815563
245.692657	8000.077841	11.257920	-0.051585	4.815574
245.691042	8000.081042	11.262925	-0.051585	4.815575
245.373275	7999.998983	11.267930	-0.051526	4.815552
245.502816	8000.029957	11.272935	-0.051550	4.815561
245.622952	8000.015922	11.277939	-0.051573	4.815556
245.408847	8000.047693	11.282944	-0.051533	4.815566
245.569237	8000.037520	11.287949	-0.051563	4.815562
245.731891	8000.046607	11.292954	-0.051594	4.815564
245.700295	8000.074950	11.297959	-0.051588	4.815573
245.573504	8000.033388	11.302963	-0.051565	4.815561
245.505083	7999.991712	11.307968	-0.051552	4.815549
245.683844	8000.046985	11.312973	-0.051586	4.815565
245.606928	8000.029733	11.317978	-0.051572	4.815560
245.692451	8000.054649	11.322983	-0.051588	4.815567
245.591048	8000.034861	11.327987	-0.051569	4.815562
245.550650	8000.055585	11.332992	-0.051562	4.815568
245.655768	8000.058393	11.337997	-0.051582	4.815568
245.487178	8000.005469	11.343002	-0.051551	4.815553
245.592139	8000.060605	11.348007	-0.051571	4.815569
245.405312	8000.045830	11.353011	-0.051536	4.815566
245.630883	8000.065557	11.358016	-0.051579	4.815570
245.691474	8000.080453	11.363021	-0.051590	4.815574
245.568234	8000.049629	11.368026	-0.051567	4.815566
245.638589	8000.081773	11.373031	-0.051581	4.815575
245.763276	8000.017618	11.378035	-0.051604	4.815556
245.662139	8000.049097	11.383040	-0.051586	4.815565
245.687185	8000.084773	11.388045	-0.051591	4.815576
245.677336	8000.052597	11.393050	-0.051589	4.815566
245.839365	8000.068082	11.398055	-0.051620	4.815570
245.637217	8000.051989	11.403059	-0.051582	4.815566
245.590988	8000.039510	11.408064	-0.051574	4.815563
245.812495	8000.022859	11.413069	-0.051615	4.815557
245.745298	8000.013241	11.418074	-0.051603	4.815554
245.817441	8000.058230	11.423079	-0.051617	4.815567
245.733227	8000.045131	11.428083	-0.051601	4.815564
245.577612	8000.072517	11.433088	-0.051573	4.815572
245.822206	8000.084010	11.438093	-0.051618	4.815575
245.612128	8000.043224	11.443098	-0.051580	4.815564
245.746496	8000.079617	11.448103	-0.051605	4.815574
245.691701	8000.044571	11.453107	-0.051595	4.815564
245.591025	8000.049359	11.458112	-0.051576	4.815566
245.841797	8000.062021	11.463117	-0.051623	4.815568
245.604298	8000.056030	11.468122	-0.051580	4.815567
245.620141	8000.086216	11.473127	-0.051583	4.815576
245.826847	8000.084275	11.478131	-0.051622	4.815575
245.843891	8000.055742	11.483136	-0.051625	4.815566
245.857938	8000.075218	11.488141	-0.051628	4.815572
245.775337	8000.050397	11.493146	-0.051613	4.815565
245.820314	8000.079991	11.498151	-0.051621	4.815573
245.681690	8000.043576	11.503155	-0.051596	4.815563
245.777935	8000.066531	11.508160	-0.051614	4.815570
245.776147	8000.081477	11.513165	-0.051614	4.815574
245.534622	8000.155520	11.518170	-0.051569	4.815597
245.654200	8000.143612	11.523175	-0.051592	4.815593
245.474510	8000.110798	11.528179	-0.051559	4.815584
245.393600	8000.074257	11.533184	-0.051544	4.815574
245.409522	8000.089492	11.538189	-0.051547	4.815578
245.557438	8000.035328	11.543194	-0.051575	4.815562
245.495536	8000.062109	11.548199	-0.051564	4.815570
245.484097	8000.035246	11.553203	-0.051562	4.815562
245.336637	8000.068105	11.558208	-0.051535	4.815572
245.510447	8000.078443	11.563213	-0.051567	4.815574
245.403730	8000.064976	11.568218	-0.051548	4.815571
245.345960	8000.071532	11.573223	-0.051537	4.815573
245.518755	8000.049814	11.578227	-0.051569	4.815566
245.721371	8000.078777	11.583232	-0.051608	4.815573
245.721619	8000.036085	11.588237	-0.051608	4.815561
245.594154	8000.059659	11.593242	-0.051584	4.815568
245.626662	8000.089049	11.598247	-0.051591	4.815577
245.459801	8000.081009	11.603251	-0.051560	4.815575
245.334151	8000.065097	11.608256	-0.051537	4.815571
245.483826	8000.054749	11.613261	-0.051565	4.815567
245.489875	8000.046327	11.618266	-0.051566	4.815565
245.337905	8000.072705	11.623271	-0.051538	4.815573
245.548132	8000.067617	11.628275	-0.051578	4.815571
245.504722	8000.073340	11.633280	-0.051570	4.815573
245.604945	8000.060048	11.638285	-0.051589	4.815568
245.549701	8000.033538	11.643290	-0.051579	4.815561
245.716299	8000.098225	11.648295	-0.051610	4.815579
245.452731	8000.077925	11.653299	-0.051561	4.815574
245.668886	8000.078275	11.658304	-0.051602	4.815573
245.788872	8000.069578	11.663309	-0.051624	4.815570
245.602805	8000.062291	11.668314	-0.051590	4.815569
245.625325	8000.086178	11.673319	-0.051594	4.815576
245.767201	8000.095994	11.678323	-0.051621	4.815578
245.717739	8000.109094	11.683328	-0.051612	4.815582
245.545170	8000.084940	11.688333	-0.051580	4.815576
245.438824	8000.040508	11.693338	-0.051561	4.815563
245.599655	8000.046362	11.698343	-0.051591	4.815564
245.520609	8000.038687	11.703347	-0.051577	4.815562
245.456844	8000.036601	11.708352	-0.051565	4.815562
245.649624	8000.068608	11.713357	-0.051601	4.815571
245.841779	8000.024778	11.718362	-0.051637	4.815557
245.762113	8000.074764	11.723367	-0.051623	4.815572
245.627432	8000.049093	11.728371	-0.051598	4.815565
245.585990	8000.091159	11.733376	-0.051590	4.815577
245.649257	8000.075128	11.738381	-0.051602	4.815572
245.508140	8000.054692	11.743386	-0.051576	4.815567
245.747225	8000.090659	11.748391	-0.051621	4.815577
245.679444	8000.045788	11.753395	-0.051609	4.815564
245.763571	8000.042914	11.758400	-0.051625	4.815562
245.965396	8000.065457	11.763405	-0.051663	4.815568
245.856149	8000.056220	11.768410	-0.051643	4.815566
245.838270	8000.087992	11.773415	-0.051640	4.815575
245.655421	8000.051922	11.778419	-0.051606	4.815566
245.646425	8000.052867	11.783424	-0.051604	4.815566
245.656494	8000.078686	11.788429	-0.051606	4.815573
245.451595	8000.055073	11.793434	-0.051569	4.815567
245.681477	8000.063122	11.798439	-0.051612	4.815569
245.710939	8000.057219	11.803443	-0.051617	4.815567
245.708721	8000.052934	11.808448	-0.051617	4.815566
245.791392	8000.076735	11.813453	-0.051633	4.815572
245.794646	8000.043705	11.818458	-0.051634	4.815562
245.890127	8000.060239	11.823463	-0.051652	4.815567
245.555921	8000.019562	11.828467	-0.051590	4.815557
245.567374	8000.031521	11.833472	-0.051592	4.815560
245.769095	8000.061538	11.838477	-0.051630	4.815568
245.660091	8000.050169	11.843482	-0.051610	4.815565
245.742437	8000.077169	11.848487	-0.051626	4.815572
245.610848	8000.059024	11.853491	-0.051601	4.815568
245.687213	8000.073111	11.858496	-0.051616	4.815572
245.709489	8000.061750	11.863501	-0.051620	4.815568
245.646812	8000.025507	11.868506	-0.051609	4.815558
245.740030	8000.000353	11.873511	-0.051627	4.815550
245.701136	7999.950615	11.878515	-0.051620	4.815536
245.947631	8000.025150	11.883520	-0.051666	4.815556
245.836360	8000.040445	11.888525	-0.051645	4.815561
245.854437	8000.031151	11.893530	-0.051649	4.815558
245.955686	8000.099044	11.898535	-0.051668	4.815578
246.182795	8000.068601	11.903539	-0.051711	4.815568
245.909885	8000.074847	11.908544	-0.051660	4.815571
245.982070	8000.055758	11.913549	-0.051674	4.815565
246.120099	8000.042016	11.918554	-0.051700	4.815560
246.095640	8000.067272	11.923559	-0.051696	4.815568
245.832569	8000.076883	11.928563	-0.051647	4.815572
245.818121	8000.063855	11.933568	-0.051644	4.815568
246.243450	8000.077233	11.938573	-0.051724	4.815570
245.920942	8000.039950	11.943578	-0.051664	4.815561
245.830939	8000.101515	11.948583	-0.051648	4.815579
245.908505	8000.056882	11.953587	-0.051662	4.815566
245.858890	8000.068911	11.958592	-0.051653	4.815569
245.867166	8000.075478	11.963597	-0.051655	4.815571
245.950848	8000.050168	11.968602	-0.051671	4.815563
245.937957	8000.093769	11.973607	-0.051669	4.815576
245.818242	8000.066206	11.978611	-0.051647	4.815569
246.080822	8000.081198	11.983616	-0.051696	4.815572
246.186819	8000.094700	11.988621	-0.051716	4.815575
246.016672	8000.052429	11.993626	-0.051685	4.815564
245.982405	8000.080729	11.998631	-0.051678	4.815572
246.156828	8000.065445	12.003635	-0.051711	4.815567
246.008260	8000.048091	12.008640	-0.051684	4.815562
245.788054	8000.071218	12.013645	-0.051643	4.815570
245.952385	8000.057905	12.018650	-0.051674	4.815566
245.927832	8000.072480	12.023655	-0.051670	4.815570
246.003026	8000.069460	12.028659	-0.051684	4.815569
245.825001	8000.069780	12.033664	-0.051651	4.815570
246.135428	8000.097301	12.038669	-0.051709	4.815576
246.079248	8000.061163	12.043674	-0.051699	4.815566
245.888421	8000.096518	12.048679	-0.051664	4.815577
246.064128	8000.081256	12.053683	-0.051697	4.815572
246.102991	8000.069098	12.058688	-0.051704	4.815568
246.244657	8000.086388	12.063693	-0.051731	4.815572
246.108914	8000.079922	12.068698	-0.051706	4.815571
246.066222	8000.089928	12.073703	-0.051698	4.815574
245.947413	8000.132868	12.078707	-0.051676	4.815587
245.774055	8000.132196	12.083712	-0.051644	4.815588
245.982355	8000.146302	12.088717	-0.051683	4.815591
245.825093	8000.067929	12.093722	-0.051654	4.815569
245.788980	8000.076975	12.098727	-0.051648	4.815572
245.937993	8000.061276	12.103731	-0.051676	4.815567
245.887588	8000.074361	12.108736	-0.051667	4.815571
245.944912	8000.094544	12.113741	-0.051678	4.815576
245.881985	8000.062568	12.118746	-0.051666	4.815567
245.814956	8000.102081	12.123751	-0.051654	4.815579
245.918566	8000.094185	12.128755	-0.051674	4.815576
245.944263	8000.108512	12.133760	-0.051679	4.815580
245.889962	8000.096969	12.138765	-0.051669	4.815577
245.926725	8000.070893	12.143770	-0.051676	4.815569
245.907086	8000.096228	12.148775	-0.051673	4.815577
245.930871	8000.073144	12.153779	-0.051677	4.815570
246.044248	8000.081427	12.158784	-0.051699	4.815572
246.041701	8000.126265	12.163789	-0.051698	4.815585
245.880117	8000.077726	12.168794	-0.051669	4.815572
245.929469	8000.099916	12.173799	-0.051678	4.815578
245.990101	8000.080638	12.178803	-0.051690	4.815572
245.898915	8000.098396	12.183808	-0.051673	4.815577
245.984382	8000.079523	12.188813	-0.051689	4.815572
245.746363	8000.064980	12.193818	-0.051645	4.815568
245.702776	8000.083516	12.198823	-0.051637	4.815574
245.788254	8000.068915	12.203827	-0.051653	4.815569
245.876734	8000.087472	12.208832	-0.051670	4.815574
245.818451	8000.083340	12.213837	-0.051660	4.815573
245.989394	8000.074407	12.218842	-0.051692	4.815570
245.999328	8000.131197	12.223847	-0.051694	4.815587
245.919530	8000.069041	12.228851	-0.051679	4.815569
245.886224	8000.069589	12.233856	-0.051673	4.815569
246.011701	8000.109042	12.238861	-0.051697	4.815580
245.927666	8000.082061	12.243866	-0.051681	4.815572
246.133938	8000.106814	12.248871	-0.051720	4.815579
245.989445	8000.062825	12.253875	-0.051694	4.815567
245.941989	8000.079162	12.258880	-0.051685	4.815572
246.021906	8000.111463	12.263885	-0.051700	4.815581
245.886634	8000.067625	12.268890	-0.051675	4.815568
245.796792	8000.083269	12.273895	-0.051659	4.815573
245.887123	8000.074088	12.278899	-0.051676	4.815570
245.916694	8000.074595	12.283904	-0.051682	4.815570
245.994949	8000.087645	12.288909	-0.051696	4.815574
245.934361	8000.053571	12.293914	-0.051685	4.815564
245.987972	8000.101462	12.298919	-0.051696	4.815578
246.067515	8000.091037	12.303923	-0.051711	4.815574
246.100236	8000.081983	12.308928	-0.051717	4.815572
246.173240	8000.105627	12.313933	-0.051731	4.815578
245.923137	8000.048166	12.318938	-0.051685	4.815562
245.970468	8000.086342	12.323943	-0.051694	4.815573
246.262924	8000.076191	12.328947	-0.051748	4.815569
246.133546	8000.062353	12.333952	-0.051725	4.815566
246.116849	8000.093076	12.338957	-0.051722	4.815575
246.070003	8000.069906	12.343962	-0.051713	4.815568
246.249580	8000.109175	12.348967	-0.051747	4.815579
245.959826	8000.032910	12.353971	-0.051693	4.815558
246.114130	8000.039726	12.358976	-0.051722	4.815559
246.352804	8000.073552	12.363981	-0.051767	4.815568
246.134144	8000.029420	12.368986	-0.051727	4.815556
246.176547	8000.061108	12.373991	-0.051735	4.815565
246.187117	8000.063441	12.378995	-0.051737	4.815566
246.249407	8000.049530	12.384000	-0.051749	4.815561
246.303104	8000.072858	12.389005	-0.051759	4.815568
246.267351	8000.046666	12.394010	-0.051753	4.815560
246.324686	8000.071122	12.399015	-0.051764	4.815567
246.235135	8000.070751	12.404019	-0.051747	4.815567
246.322114	8000.076467	12.409024	-0.051764	4.815569
246.393722	8000.087273	12.414029	-0.051777	4.815572
246.075709	8000.038314	12.419034	-0.051718	4.815559
246.109115	8000.080535	12.424039	-0.051725	4.815571
246.223687	8000.069614	12.429043	-0.051747	4.815567
245.977962	8000.048536	12.434048	-0.051701	4.815562
246.030589	8000.093208	12.439053	-0.051711	4.815575
246.207913	8000.057679	12.444058	-0.051744	4.815564
246.289405	8000.096414	12.449063	-0.051760	4.815575
246.185278	8000.106485	12.454067	-0.051741	4.815578
246.224335	8000.083651	12.459072	-0.051748	4.815571
246.321254	8000.078849	12.464077	-0.051767	4.815569
246.360240	8000.083782	12.469082	-0.051774	4.815571
246.283301	8000.095365	12.474087	-0.051760	4.815574
246.380901	8000.083099	12.479091	-0.051779	4.815570
246.149026	8000.071859	12.484096	-0.051736	4.815568
246.253849	8000.076799	12.489101	-0.051755	4.815569
246.177531	8000.060624	12.494106	-0.051741	4.815565
246.216981	8000.082652	12.499111	-0.051749	4.815571
246.091204	8000.080621	12.504115	-0.051726	4.815571
246.326195	8000.088755	12.509120	-0.051770	4.815572
246.339841	8000.117838	12.514125	-0.051773	4.815581
246.083406	8000.132897	12.519130	-0.051725	4.815586
246.150004	8000.175660	12.524135	-0.051738	4.815598
246.078600	8000.140341	12.529139	-0.051725	4.815588
246.044837	8000.106705	12.534144	-0.051719	4.815579
245.999630	8000.139099	12.539149	-0.051711	4.815588
246.203866	8000.101874	12.544154	-0.051749	4.815577
246.152245	8000.103191	12.549159	-0.051740	4.815577
246.135686	8000.094400	12.554163	-0.051737	4.815575
246.004224	8000.084800	12.559168	-0.051713	4.815572
246.036829	8000.108852	12.564173	-0.051719	4.815579
246.197353	8000.067710	12.569178	-0.051749	4.815567
246.030736	8000.079964	12.574183	-0.051718	4.815571
246.314598	8000.062196	12.579187	-0.051772	4.815564
246.204977	8000.084993	12.584192	-0.051751	4.815572
246.258989	8000.108327	12.589197	-0.051762	4.815578
246.245507	8000.073955	12.594202	-0.051760	4.815568
246.109644	8000.079235	12.599207	-0.051735	4.815570
246.189763	8000.091247	12.604211	-0.051750	4.815573
246.144140	8000.077710	12.609216	-0.051741	4.815570
246.036469	8000.127239	12.614221	-0.051722	4.815585
245.984739	8000.129622	12.619226	-0.051712	4.815586
245.897599	8000.106862	12.624231	-0.051696	4.815579
246.155931	8000.145281	12.629235	-0.051745	4.815589
246.108172	8000.083648	12.634240	-0.051736	4.815572
246.131024	8000.132106	12.639245	-0.051741	4.815586
246.269371	8000.102349	12.644250	-0.051767	4.815576
246.257401	8000.129945	12.649255	-0.051765	4.815584
246.132915	8000.103371	12.654259	-0.051742	4.815577
246.008223	8000.098154	12.659264	-0.051719	4.815576
246.370549	8000.095552	12.664269	-0.051787	4.815574
246.286941	8000.073918	12.669274	-0.051771	4.815568
246.133564	8000.098136	12.674279	-0.051743	4.815576
246.140305	8000.086522	12.679283	-0.051745	4.815572
245.952550	8000.067459	12.684288	-0.051710	4.815567
246.012247	8000.075934	12.689293	-0.051721	4.815570
246.076213	8000.062050	12.694298	-0.051733	4.815565
246.136202	8000.084414	12.699303	-0.051745	4.815572
246.086605	8000.076151	12.704307	-0.051736	4.815569
245.977415	8000.073323	12.709312	-0.051716	4.815569
246.114919	8000.096953	12.714317	-0.051742	4.815575
246.194047	8000.092929	12.719322	-0.051757	4.815574
246.094638	8000.094533	12.724327	-0.051738	4.815575
245.958906	8000.069911	12.729331	-0.051713	4.815568
246.151840	8000.073086	12.734336	-0.051750	4.815568
246.237689	8000.087328	12.739341	-0.051766	4.815572
246.000852	8000.071735	12.744346	-0.051722	4.815568
246.124895	8000.101553	12.749351	-0.051745	4.815577
246.097906	8000.071232	12.754355	-0.051741	4.815568
245.897689	8000.064781	12.759360	-0.051704	4.815567
246.040741	8000.128018	12.764365	-0.051731	4.815585
246.033021	8000.086263	12.769370	-0.051729	4.815572
246.044040	8000.095011	12.774375	-0.051732	4.815575
246.070134	8000.115753	12.779379	-0.051737	4.815581
246.127484	8000.091081	12.784384	-0.051748	4.815573
246.167911	8000.088561	12.789389	-0.051756	4.815572
246.069416	8000.068820	12.794394	-0.051738	4.815567
246.259670	8000.081563	12.799399	-0.051773	4.815570
246.188543	8000.086833	12.804403	-0.051760	4.815572
246.022947	8000.084152	12.809408	-0.051730	4.815572
246.281627	8000.105489	12.814413	-0.051778	4.815577
246.346469	8000.088416	12.819418	-0.051790	4.815572
246.244434	8000.122017	12.824423	-0.051772	4.815582
246.222782	8000.093918	12.829427	-0.051768	4.815574
246.268463	8000.087212	12.834432	-0.051777	4.815572
246.348122	8000.103489	12.839437	-0.051792	4.815576
246.175961	8000.075068	12.844442	-0.051760	4.815568
246.253625	8000.092381	12.849447	-0.051775	4.815573
246.186798	8000.089177	12.854451	-0.051763	4.815572
246.046190	8000.095448	12.859456	-0.051737	4.815575
246.045151	8000.106134	12.864461	-0.051737	4.815578
246.089365	8000.054548	12.869466	-0.051745	4.815563
246.256693	8000.060509	12.874471	-0.051777	4.815564
246.169455	8000.080468	12.879475	-0.051761	4.815570
246.146830	8000.090802	12.884480	-0.051757	4.815573
246.284582	8000.111232	12.889485	-0.051783	4.815578
246.270935	8000.101420	12.894490	-0.051780	4.815576
246.218988	8000.105935	12.899495	-0.051771	4.815577
246.189896	8000.100144	12.904499	-0.051766	4.815576
246.062779	8000.076731	12.909504	-0.051742	4.815569
246.364070	8000.109444	12.914509	-0.051799	4.815577
246.372395	8000.094652	12.919514	-0.051801	4.815573
246.243901	8000.127821	12.924519	-0.051777	4.815583
246.062314	8000.165462	12.929523	-0.051744	4.815595
246.088306	8000.110374	12.934528	-0.051749	4.815579
246.242420	8000.134276	12.939533	-0.051778	4.815585
246.154748	8000.106167	12.944538	-0.051762	4.815577
246.153469	8000.095489	12.949543	-0.051762	4.815574
246.119845	8000.067196	12.954547	-0.051756	4.815566
246.056005	8000.064040	12.959552	-0.051744	4.815566
246.345975	8000.120065	12.964557	-0.051798	4.815581
246.264804	8000.068566	12.969562	-0.051783	4.815566
246.254835	8000.092991	12.974567	-0.051782	4.815573
246.223663	8000.105322	12.979571	-0.051776	4.815577
246.198796	8000.075035	12.984576	-0.051772	4.815568
246.562854	8000.071394	12.989581	-0.051840	4.815565
246.368408	8000.085329	12.994586	-0.051804	4.815570
246.450177	8000.104845	12.999591	-0.051819	4.815576
246.403586	8000.076339	13.004595	-0.051811	4.815567
246.258532	8000.095353	13.009600	-0.051784	4.815574
246.221696	8000.108659	13.014605	-0.051778	4.815578
246.239613	8000.070527	13.019610	-0.051781	4.815567
246.376803	8000.101628	13.024615	-0.051807	4.815575
246.053517	8000.122003	13.029619	-0.051747	4.815582
246.434110	8000.110088	13.034624	-0.051818	4.815577
246.613788	8000.113047	13.039629	-0.051852	4.815577
246.277306	8000.086213	13.044634	-0.051790	4.815571
246.028823	8000.104606	13.049639	-0.051744	4.815577
246.204433	8000.079730	13.054643	-0.051777	4.815569
246.286939	8000.090714	13.059648	-0.051792	4.815572
246.472388	8000.143964	13.064653	-0.051827	4.815587
246.491491	8000.141096	13.069658	-0.051831	4.815586
246.394137	8000.117100	13.074663	-0.051813	4.815579
246.451592	8000.107382	13.079667	-0.051824	4.815576
246.274465	8000.075676	13.084672	-0.051791	4.815568
246.237608	8000.102866	13.089677	-0.051785	4.815576
246.258357	8000.078664	13.094682	-0.051789	4.815569
246.317889	8000.104225	13.099687	-0.051800	4.815576
246.191652	8000.098982	13.104691	-0.051777	4.815575
246.259967	8000.062741	13.109696	-0.051790	4.815564
246.056486	8000.090413	13.114701	-0.051752	4.815573
246.230300	8000.069780	13.119706	-0.051785	4.815566
246.365088	8000.113658	13.124711	-0.051810	4.815578
246.422936	8000.103946	13.129715	-0.051821	4.815575
246.349485	8000.077138	13.134720	-0.051808	4.815568
246.541464	8000.120883	13.139725	-0.051844	4.815580
246.467351	8000.088723	13.144730	-0.051830	4.815571
246.405079	8000.094137	13.149735	-0.051819	4.815572
246.554851	8000.078451	13.154739	-0.051847	4.815567
246.372736	8000.072296	13.159744	-0.051814	4.815566
246.463674	8000.099437	13.164749	-0.051831	4.815574
246.382368	8000.071432	13.169754	-0.051816	4.815566
246.325043	8000.100424	13.174759	-0.051806	4.815575
246.524563	8000.085551	13.179763	-0.051843	4.815569
246.168546	8000.056262	13.184768	-0.051777	4.815562
246.357797	8000.101030	13.189773	-0.051813	4.815575
246.270836	8000.086817	13.194778	-0.051797	4.815571
246.180837	8000.132363	13.199783	-0.051780	4.815585
246.325849	8000.099511	13.204787	-0.051807	4.815574
246.292371	8000.081899	13.209792	-0.051801	4.815569
246.367400	8000.095965	13.214797	-0.051816	4.815573
246.588925	8000.066499	13.219802	-0.051857	4.815563
246.534655	8000.106221	13.224807	-0.051847	4.815575
246.691882	8000.093861	13.229811	-0.051877	4.815571
246.410402	8000.101034	13.234816	-0.051825	4.815574
246.530123	8000.100878	13.239821	-0.051847	4.815574
246.336732	8000.060361	13.244826	-0.051812	4.815563
246.239940	8000.078028	13.249831	-0.051794	4.815568
246.357666	8000.086383	13.254835	-0.051816	4.815570
246.385047	8000.068698	13.259840	-0.051821	4.815565
246.333343	8000.093509	13.264845	-0.051812	4.815572
246.204011	8000.066855	13.269850	-0.051788	4.815565
246.375714	8000.095316	13.274855	-0.051820	4.815573
246.278768	8000.082008	13.279859	-0.051803	4.815569
246.284009	8000.087457	13.284864	-0.051804	4.815571
246.419564	8000.099308	13.289869	-0.051829	4.815574
246.409180	8000.085278	13.294874	-0.051828	4.815570
246.298481	8000.094173	13.299879	-0.051807	4.815573
246.615068	8000.083348	13.304883	-0.051867	4.815568
246.609283	8000.065121	13.309888	-0.051866	4.815563
246.722680	8000.105447	13.314893	-0.051887	4.815574
246.557690	8000.064326	13.319898	-0.051857	4.815563
246.600403	8000.112040	13.324903	-0.051865	4.815577
246.581779	8000.102147	13.329907	-0.051862	4.815574
246.533574	8000.077887	13.334912	-0.051853	4.815567
246.615849	8000.117703	13.339917	-0.051869	4.815578
246.528019	8000.097068	13.344922	-0.051853	4.815572
246.313678	8000.113882	13.349927	-0.051813	4.815578
246.278497	8000.096242	13.354931	-0.051807	4.815573
246.241752	8000.076442	13.359936	-0.051800	4.815568
246.468401	8000.057740	13.364941	-0.051843	4.815561
246.322939	8000.058591	13.369946	-0.051816	4.815562
246.409184	8000.094200	13.374951	-0.051832	4.815572
246.755979	8000.112706	13.379955	-0.051897	4.815576
246.549478	8000.075179	13.384960	-0.051859	4.815566
246.570595	8000.110792	13.389965	-0.051863	4.815576
246.582882	8000.086452	13.394970	-0.051865	4.815569
246.624787	8000.110657	13.399975	-0.051874	4.815576
246.708851	8000.133415	13.404979	-0.051889	4.815582
246.642469	8000.107789	13.409984	-0.051877	4.815575
246.570635	8000.098095	13.414989	-0.051864	4.815572
246.372656	8000.125856	13.419994	-0.051828	4.815582
246.487381	8000.123482	13.424999	-0.051849	4.815580
246.368894	8000.119434	13.430003	-0.051828	4.815580
246.268734	8000.088985	13.435008	-0.051809	4.815571
246.568330	8000.112060	13.440013	-0.051865	4.815577
246.680334	8000.138478	13.445018	-0.051886	4.815584
246.698946	8000.111037	13.450023	-0.051890	4.815576
246.699988	8000.133506	13.455027	-0.051891	4.815582
246.779497	8000.102788	13.460032	-0.051906	4.815573
246.838677	8000.116596	13.465037	-0.051917	4.815577
246.602821	8000.090337	13.470042	-0.051873	4.815570
246.814369	8000.111973	13.475047	-0.051913	4.815575
246.822413	8000.117469	13.480051	-0.051915	4.815577
246.730497	8000.081813	13.485056	-0.051898	4.815567
246.603968	8000.115015	13.490061	-0.051875	4.815577
246.416254	8000.091679	13.495066	-0.051840	4.815571
246.421869	8000.080046	13.500071	-0.051841	4.815568
246.604526	8000.115095	13.505075	-0.051875	4.815577
246.632726	8000.072858	13.510080	-0.051881	4.815565
246.669280	8000.106588	13.515085	-0.051888	4.815574
246.529173	8000.089370	13.520090	-0.051862	4.815570
246.484954	8000.079059	13.525095	-0.051854	4.815567
246.554388	8000.082353	13.530099	-0.051867	4.815568
246.234145	8000.056852	13.535104	-0.051808	4.815562
246.411749	8000.120654	13.540109	-0.051841	4.815580
246.675276	8000.097215	13.545114	-0.051891	4.815572
246.541606	8000.074762	13.550119	-0.051866	4.815566
246.463141	8000.080980	13.555123	-0.051852	4.815568
246.497958	8000.086913	13.560128	-0.051859	4.815569
246.760088	8000.110444	13.565133	-0.051908	4.815575
246.660055	8000.073588	13.570138	-0.051889	4.815565
246.487565	8000.094290	13.575143	-0.051857	4.815572
246.510055	8000.096817	13.580147	-0.051862	4.815572
246.403379	8000.079078	13.585152	-0.051842	4.815567
246.383778	8000.063829	13.590157	-0.051839	4.815563
246.287012	8000.081496	13.595162	-0.051821	4.815569
246.323191	8000.087451	13.600167	-0.051828	4.815570
246.510807	8000.090540	13.605171	-0.051863	4.815570
246.505804	8000.058441	13.610176	-0.051863	4.815561
246.560408	8000.099941	13.615181	-0.051873	4.815573
246.498708	8000.061576	13.620186	-0.051862	4.815562
246.486618	8000.078491	13.625191	-0.051860	4.815567
246.763097	8000.104392	13.630195	-0.051912	4.815573
246.709630	8000.093930	13.635200	-0.051902	4.815570
246.441743	8000.102393	13.640205	-0.051852	4.815574
246.316340	8000.075803	13.645210	-0.051829	4.815567
246.562839	8000.081990	13.650215	-0.051875	4.815567
246.501641	8000.079946	13.655219	-0.051864	4.815567
246.593017	8000.049422	13.660224	-0.051882	4.815558
246.621363	8000.092630	13.665229	-0.051887	4.815570
246.312500	8000.079063	13.670234	-0.051830	4.815568
246.291653	8000.090494	13.675239	-0.051826	4.815571
246.532055	8000.109398	13.680243	-0.051871	4.815576
246.525264	8000.094358	13.685248	-0.051870	4.815571
246.437936	8000.110043	13.690253	-0.051854	4.815576
246.547235	8000.093696	13.695258	-0.051875	4.815571
246.517420	8000.092165	13.700263	-0.051870	4.815571
246.677686	8000.117236	13.705267	-0.051900	4.815577
246.683859	8000.081047	13.710272	-0.051901	4.815567
246.850450	8000.110494	13.715277	-0.051933	4.815574
246.534697	8000.089338	13.720282	-0.051874	4.815570
246.546738	8000.083150	13.725287	-0.051877	4.815568
246.617388	8000.105688	13.730291	-0.051890	4.815574
246.427740	8000.073777	13.735296	-0.051855	4.815566
246.397439	8000.076509	13.740301	-0.051850	4.815567
246.661388	8000.081914	13.745306	-0.051899	4.815567
246.674073	8000.108845	13.750311	-0.051902	4.815575
246.497092	8000.117725	13.755315	-0.051869	4.815578
246.419094	8000.117543	13.760320	-0.051855	4.815578
246.837279	8000.061386	13.765325	-0.051933	4.815560
246.713609	8000.056184	13.770330	-0.051910	4.815559
246.789353	8000.068126	13.775335	-0.051924	4.815562
246.751556	8000.086757	13.780339	-0.051918	4.815568
246.694179	8000.048462	13.785344	-0.051907	4.815557
246.774317	8000.107468	13.790349	-0.051922	4.815574
246.760905	8000.097661	13.795354	-0.051920	4.815571
246.783167	8000.098048	13.800359	-0.051925	4.815571
246.764636	8000.098837	13.805363	-0.051921	4.815571
246.702487	8000.069008	13.810368	-0.051910	4.815563
246.825917	8000.109498	13.815373	-0.051933	4.815574
246.917532	8000.077910	13.820378	-0.051951	4.815564
246.765543	8000.094674	13.825383	-0.051923	4.815570
246.830854	8000.145963	13.830387	-0.051935	4.815585
246.628507	8000.089278	13.835392	-0.051898	4.815569
246.476196	8000.085745	13.840397	-0.051870	4.815569
246.583174	8000.088585	13.845402	-0.051890	4.815569
246.641942	8000.092773	13.850407	-0.051901	4.815570
246.606608	8000.111443	13.855411	-0.051895	4.815576
246.583665	8000.063031	13.860416	-0.051891	4.815562
246.779918	8000.105779	13.865421	-0.051927	4.815573
246.772360	8000.100338	13.870426	-0.051926	4.815572
246.622205	8000.102181	13.875431	-0.051899	4.815573
246.671366	8000.104076	13.880435	-0.051908	4.815573
246.579727	8000.064153	13.885440	-0.051891	4.815562
246.727801	8000.122134	13.890445	-0.051919	4.815578
246.743981	8000.078632	13.895450	-0.051922	4.815565
246.870131	8000.075377	13.900455	-0.051946	4.815564
246.844441	8000.078185	13.905459	-0.051942	4.815565
246.672535	8000.089284	13.910464	-0.051910	4.815569
246.854616	8000.109372	13.915469	-0.051944	4.815574
246.879990	8000.066021	13.920474	-0.051949	4.815561
246.603016	8000.080743	13.925479	-0.051898	4.815567
246.810740	8000.109794	13.930483	-0.051937	4.815574
246.866949	8000.111804	13.935488	-0.051947	4.815574
246.740345	8000.106555	13.940493	-0.051924	4.815573
246.557140	8000.074748	13.945498	-0.051890	4.815565
246.582029	8000.102947	13.950503	-0.051895	4.815573
246.755363	8000.106871	13.955507	-0.051928	4.815573
246.501394	8000.083520	13.960512	-0.051881	4.815568
246.884479	8000.130389	13.965517	-0.051952	4.815580
246.710148	8000.115815	13.970522	-0.051920	4.815576
246.616458	8000.107900	13.975527	-0.051903	4.815574
246.818202	8000.109084	13.980531	-0.051941	4.815574
246.796931	8000.114100	13.985536	-0.051937	4.815575
246.788011	8000.108638	13.990541	-0.051936	4.815574
246.794026	8000.102352	13.995546	-0.051937	4.815572
246.883127	8000.093151	14.000551	-0.051954	4.815569
246.894591	8000.116859	14.005555	-0.051956	4.815576
246.837869	8000.101003	14.010560	-0.051946	4.815571
246.882910	8000.119919	14.015565	-0.051955	4.815577
246.995558	8000.104695	14.020570	-0.051976	4.815572
246.654207	8000.084188	14.025575	-0.051913	4.815567
246.857627	8000.122781	14.030579	-0.051951	4.815577
246.737071	8000.111222	14.035584	-0.051929	4.815575
246.743094	8000.132705	14.040589	-0.051930	4.815581
246.648255	8000.108750	14.045594	-0.051913	4.815574
246.771759	8000.097976	14.050599	-0.051936	4.815571
246.848346	8000.131292	14.055603	-0.051950	4.815580
246.654891	8000.093977	14.060608	-0.051915	4.815570
246.687986	8000.135127	14.065613	-0.051921	4.815582
246.830476	8000.104370	14.070618	-0.051948	4.815572
246.581630	8000.099259	14.075623	-0.051902	4.815572
246.465650	8000.119816	14.080627	-0.051881	4.815578
246.599967	8000.088926	14.085632	-0.051906	4.815569
246.675453	8000.159605	14.090637	-0.051920	4.815589
246.594558	8000.193552	14.095642	-0.051905	4.815599
246.518679	8000.142138	14.100647	-0.051892	4.815585
246.763549	8000.156844	14.105651	-0.051937	4.815588
246.622278	8000.090477	14.110656	-0.051911	4.815569
246.822005	8000.114057	14.115661	-0.051949	4.815575
246.738270	8000.106304	14.120666	-0.051933	4.815573
246.542746	8000.121289	14.125671	-0.051897	4.815578
246.474991	8000.106321	14.130675	-0.051885	4.815574
246.655776	8000.092210	14.135680	-0.051919	4.815569
246.618339	8000.135411	14.140685	-0.051912	4.815582
246.677904	8000.099027	14.145690	-0.051924	4.815571
246.866601	8000.099999	14.150695	-0.051959	4.815571
246.855885	8000.113732	14.155699	-0.051957	4.815575
246.468383	8000.105287	14.160704	-0.051885	4.815574
246.465147	8000.107394	14.165709	-0.051885	4.815575
246.810666	8000.093839	14.170714	-0.051950	4.815569
246.703574	8000.089976	14.175719	-0.051930	4.815568
246.563936	8000.126167	14.180723	-0.051904	4.815580
246.390035	8000.108397	14.185728	-0.051872	4.815575
246.530717	8000.114991	14.190733	-0.051899	4.815577
246.522261	8000.119149	14.195738	-0.051897	4.815578
246.581961	8000.089175	14.200743	-0.051909	4.815569
246.577266	8000.104075	14.205747	-0.051908	4.815573
246.595762	8000.079836	14.210752	-0.051912	4.815566
246.842526	8000.092436	14.215757	-0.051958	4.815568
246.921275	8000.099087	14.220762	-0.051973	4.815570
246.793840	8000.091688	14.225767	-0.051949	4.815568
246.651803	8000.109683	14.230771	-0.051923	4.815574
246.663914	8000.060775	14.235776	-0.051926	4.815560
246.727975	8000.087478	14.240781	-0.051938	4.815567
246.553138	8000.075033	14.245786	-0.051906	4.815565
246.507400	8000.087125	14.250791	-0.051897	4.815568
246.668041	8000.110067	14.255795	-0.051928	4.815574
246.537182	7999.314426	14.260800	-0.051903	4.815342

246.436257	7996.021636	14.265805	-0.051882	4.814380
246.639841	7990.564254	14.270810	-0.051917	4.812783
246.643231	7983.882636	14.275815	-0.051914	4.810829
246.563375	7976.628637	14.280819	-0.051894	4.808706
246.445024	7968.980717	14.285824	-0.051867	4.806467
246.354997	7961.219643	14.290829	-0.051846	4.804194
246.404174	7953.417541	14.295834	-0.051850	4.801907
246.313315	7945.362634	14.300839	-0.051828	4.799546
246.302251	7937.443781	14.305843	-0.051821	4.797223
246.339244	7929.410377	14.310848	-0.051823	4.794865
246.318552	7921.405595	14.315853	-0.051815	4.792514
246.264106	7913.328847	14.320858	-0.051799	4.790141
246.217247	7905.404895	14.325863	-0.051786	4.787812
246.311710	7897.403999	14.330867	-0.051798	4.785459
246.015048	7889.420762	14.335872	-0.051738	4.783111
246.120029	7881.431071	14.340877	-0.051753	4.780759
246.172682	7873.496514	14.345882	-0.051758	4.778422
245.963061	7865.398215	14.350887	-0.051714	4.776036
246.078865	7857.415173	14.355891	-0.051730	4.773682
246.046264	7849.377007	14.360896	-0.051719	4.771311
245.959115	7841.332657	14.365901	-0.051698	4.768938
245.991552	7833.387908	14.370906	-0.051699	4.766592
245.911933	7825.317861	14.375911	-0.051679	4.764208
245.952409	7817.479321	14.380915	-0.051682	4.761891
245.816694	7809.373357	14.385920	-0.051652	4.759495
245.632363	7801.414457	14.390925	-0.051613	4.757141
245.524732	7793.383467	14.395930	-0.051588	4.754764
245.351791	7785.262013	14.400935	-0.051550	4.752359
245.375194	7777.338615	14.405939	-0.051550	4.750012
245.299519	7769.324360	14.410944	-0.051531	4.747636
245.380938	7761.300027	14.415949	-0.051541	4.745256
245.488564	7753.370426	14.420954	-0.051556	4.742903
245.182891	7745.326982	14.425959	-0.051494	4.740515
245.149064	7737.392353	14.430963	-0.051483	4.738159
245.082684	7729.312239	14.435968	-0.051466	4.735758
245.363677	7721.326713	14.440973	-0.051513	4.733382
245.283266	7713.347996	14.445978	-0.051493	4.731009
245.068395	7705.304970	14.450983	-0.051448	4.728616
245.230725	7697.344969	14.455987	-0.051474	4.726245
245.397588	7689.272666	14.460992	-0.051500	4.723839
245.081126	7681.317522	14.465997	-0.051436	4.721469
245.179006	7673.328133	14.471002	-0.051449	4.719086
245.222544	7665.363223	14.476007	-0.051452	4.716709
245.015403	7657.319802	14.481011	-0.051409	4.714308
245.087485	7649.298431	14.486016	-0.051417	4.711912
244.869262	7641.247566	14.491021	-0.051372	4.709506
244.916294	7633.339633	14.496026	-0.051375	4.707142
244.891875	7625.299509	14.501031	-0.051366	4.704737
244.581399	7617.340744	14.506035	-0.051303	4.702355
244.384398	7609.267058	14.511040	-0.051261	4.699938
244.557316	7601.358426	14.516045	-0.051289	4.697568
244.559306	7593.295394	14.521050	-0.051284	4.695151
244.650045	7585.295358	14.526055	-0.051296	4.692751
244.608187	7577.267374	14.531059	-0.051283	4.690342
244.534991	7569.285977	14.536064	-0.051265	4.687946
244.592164	7561.250215	14.541069	-0.051270	4.685532
244.426531	7553.316009	14.546074	-0.051235	4.683148
244.220437	7545.265293	14.551079	-0.051191	4.680728
244.363044	7537.319178	14.556083	-0.051213	4.678337
244.474677	7529.300192	14.561088	-0.051229	4.675923
244.517206	7521.264257	14.566093	-0.051232	4.673503
244.473591	7513.184434	14.571098	-0.051219	4.671068
244.164219	7505.157385	14.576103	-0.051156	4.668649
244.286007	7497.246106	14.581107	-0.051174	4.666262
244.036207	7489.204977	14.586112	-0.051122	4.663836
244.162766	7481.255355	14.591117	-0.051141	4.661435
244.307912	7473.249932	14.596122	-0.051163	4.659017
244.046922	7465.194575	14.601127	-0.051110	4.656582
244.206081	7457.197521	14.606131	-0.051134	4.654163
244.110457	7449.231655	14.611136	-0.051112	4.651753
244.238980	7441.214920	14.616141	-0.051131	4.649326
244.166887	7433.292484	14.621146	-0.051112	4.646927
244.284386	7425.176889	14.626151	-0.051129	4.644467
244.172906	7417.287392	14.631155	-0.051103	4.642075
243.947777	7409.218645	14.636160	-0.051057	4.639627
243.787525	7401.266456	14.641165	-0.051022	4.637214
243.760886	7393.216949	14.646170	-0.051012	4.634769
243.715296	7385.162435	14.651175	-0.050998	4.632322
243.819720	7377.204792	14.656179	-0.051013	4.629903
243.764175	7369.210060	14.661184	-0.050998	4.627471
243.657467	7361.184645	14.666189	-0.050973	4.625029
243.577127	7353.215813	14.671194	-0.050953	4.622602
243.510203	7345.171300	14.676199	-0.050935	4.620151
243.746757	7337.232551	14.681203	-0.050975	4.617731
243.420826	7329.176035	14.686208	-0.050909	4.615274
243.491353	7321.187325	14.691213	-0.050917	4.612837
243.487248	7313.151724	14.696218	-0.050911	4.610384
243.464280	7305.145963	14.701223	-0.050902	4.607938
243.382216	7297.145529	14.706227	-0.050882	4.605493
243.231678	7289.195375	14.711232	-0.050849	4.603062
243.274966	7281.159508	14.716237	-0.050852	4.600603
243.366684	7273.171710	14.721242	-0.050864	4.598158
243.128436	7265.145811	14.726247	-0.050815	4.595700
243.212924	7257.165535	14.731251	-0.050826	4.593254
243.061340	7249.124768	14.736256	-0.050793	4.590789
243.021299	7241.116649	14.741261	-0.050780	4.588332
242.967627	7233.110838	14.746266	-0.050765	4.585875
242.982001	7225.117313	14.751271	-0.050763	4.583420
242.958258	7217.153567	14.756275	-0.050754	4.580973
242.787879	7209.108211	14.761280	-0.050717	4.578499
242.757759	7201.117589	14.766285	-0.050706	4.576041
242.648031	7193.124436	14.771290	-0.050681	4.573581
242.608617	7185.086743	14.776295	-0.050669	4.571106
242.679298	7177.091529	14.781299	-0.050677	4.568643
242.570562	7169.136720	14.786304	-0.050652	4.566191
242.566821	7161.124091	14.791309	-0.050646	4.563719
242.678945	7153.182080	14.796314	-0.050662	4.561268
242.581266	7145.099655	14.801319	-0.050639	4.558773
242.553448	7137.192122	14.806323	-0.050629	4.556330
242.396916	7129.127901	14.811328	-0.050595	4.553837
242.411989	7121.084473	14.816333	-0.050593	4.551349
242.390008	7113.111197	14.821338	-0.050583	4.548882
242.271419	7105.119590	14.826343	-0.050556	4.546407
242.367143	7097.125161	14.831347	-0.050569	4.543931
242.248486	7089.145348	14.836352	-0.050542	4.541457
242.265670	7081.112775	14.841357	-0.050541	4.538966
242.184832	7073.158638	14.846362	-0.050521	4.536498
242.294001	7065.072961	14.851367	-0.050536	4.533988
242.393128	7057.116384	14.856371	-0.050549	4.531517
242.196324	7049.083746	14.861376	-0.050508	4.529020
242.172899	7041.118666	14.866381	-0.050499	4.526543
242.226616	7033.127324	14.871386	-0.050504	4.524056
242.163915	7025.141207	14.876391	-0.050487	4.521570
242.142487	7017.107104	14.881395	-0.050478	4.519067
241.819781	7009.154879	14.886400	-0.050413	4.516588
241.787365	7001.093780	14.891405	-0.050402	4.514074
241.782047	6993.007965	14.896410	-0.050396	4.511552
241.588415	6984.997217	14.901415	-0.050355	4.509050
241.675111	6977.059579	14.906419	-0.050366	4.506571
241.542699	6969.050276	14.911424	-0.050337	4.504067
241.709390	6961.086767	14.916429	-0.050363	4.501578
241.716581	6953.087145	14.921434	-0.050359	4.499075
241.567866	6945.102387	14.926439	-0.050327	4.496575
241.535268	6937.086170	14.931443	-0.050316	4.494064
241.666095	6929.010147	14.936448	-0.050335	4.491533
241.537405	6921.022786	14.941453	-0.050306	4.489028
241.682415	6913.085955	14.946458	-0.050328	4.486538
241.507439	6905.029476	14.951463	-0.050291	4.484008
241.400718	6897.119997	14.956467	-0.050266	4.481523
241.197023	6889.020340	14.961472	-0.050223	4.478977
241.340704	6881.051663	14.966477	-0.050245	4.476472
241.195798	6873.048894	14.971482	-0.050213	4.473953
241.097688	6864.984743	14.976487	-0.050190	4.471414
241.134977	6857.008896	14.981491	-0.050192	4.468902
241.060546	6849.020989	14.986496	-0.050173	4.466384
241.068205	6841.014889	14.991501	-0.050169	4.463859
241.136886	6833.066999	14.996506	-0.050177	4.461352
241.063317	6824.989844	15.001511	-0.050158	4.458801
240.858741	6817.059256	15.006515	-0.050115	4.456295
240.723987	6809.007925	15.011520	-0.050085	4.453750
240.652059	6800.986121	15.016525	-0.050067	4.451213
240.774211	6792.993057	15.021530	-0.050085	4.448684
240.865456	6785.020675	15.026535	-0.050097	4.446160
240.849239	6777.009882	15.031539	-0.050089	4.443622
240.879116	6769.048353	15.036544	-0.050090	4.441099
240.689664	6761.033325	15.041549	-0.050049	4.438556
240.567224	6753.004343	15.046554	-0.050022	4.436007
240.498039	6744.969455	15.051559	-0.050004	4.433456
240.292660	6736.953936	15.056563	-0.049960	4.430908
240.264496	6728.943505	15.061568	-0.049950	4.428361
240.250315	6720.957120	15.066573	-0.049943	4.425821
240.302079	6712.977299	15.071578	-0.049947	4.423282
240.206518	6705.008179	15.076583	-0.049925	4.420743
240.387671	6697.007150	15.081587	-0.049953	4.418195
240.270001	6688.947725	15.086592	-0.049927	4.415625
239.979795	6680.961289	15.091597	-0.049868	4.413076
239.895857	6672.949933	15.096602	-0.049847	4.410518
240.097509	6664.923065	15.101607	-0.049880	4.407956
240.072964	6656.978680	15.106611	-0.049870	4.405417
240.060636	6648.964505	15.111616	-0.049863	4.402854
240.026598	6641.000244	15.116621	-0.049852	4.400306
239.811997	6633.029992	15.121626	-0.049807	4.397754
239.617860	6624.991032	15.126631	-0.049766	4.395178
239.863244	6616.992186	15.131635	-0.049806	4.392615
239.883696	6608.946339	15.136640	-0.049805	4.390035
239.667469	6600.976486	15.141645	-0.049760	4.387477
239.596048	6592.959231	15.146650	-0.049742	4.384902
239.673545	6584.992630	15.151655	-0.049751	4.382344
239.577191	6576.935737	15.156659	-0.049728	4.379753
239.282349	6568.986270	15.161664	-0.049669	4.377195
239.269232	6560.995633	15.166669	-0.049661	4.374623
239.446603	6552.989669	15.171674	-0.049689	4.372046
239.388251	6544.951160	15.176679	-0.049673	4.369456
239.388525	6536.996683	15.181683	-0.049669	4.366892
239.263282	6528.960291	15.186688	-0.049640	4.364298
239.139152	6521.032176	15.191693	-0.049612	4.361739
239.125519	6512.986767	15.196698	-0.049605	4.359140
239.190979	6505.016069	15.201703	-0.049612	4.356565
239.322682	6496.929048	15.206707	-0.049632	4.353951
239.151045	6488.861659	15.211712	-0.049595	4.351340
239.022945	6480.833006	15.216717	-0.049566	4.348740
239.099932	6472.907114	15.221722	-0.049575	4.346173
238.940198	6464.957108	15.226727	-0.049541	4.343595
238.902559	6456.973719	15.231731	-0.049529	4.341006
238.920257	6448.936235	15.236736	-0.049527	4.338397
238.979617	6440.934414	15.241741	-0.049533	4.335800
238.789373	6432.943722	15.246746	-0.049493	4.333202
238.811408	6424.887038	15.251751	-0.049492	4.330583
238.804161	6416.955802	15.256755	-0.049486	4.328003
238.654990	6408.944235	15.261760	-0.049453	4.325394
238.582985	6400.966508	15.266765	-0.049434	4.322796
238.605785	6392.968490	15.271770	-0.049434	4.320189
238.490903	6384.950673	15.276775	-0.049407	4.317574
238.605927	6376.928665	15.281779	-0.049424	4.314957
238.429775	6368.945947	15.286784	-0.049386	4.312350
238.430358	6360.873247	15.291789	-0.049381	4.309713
238.298293	6352.959478	15.296794	-0.049352	4.307125
238.418046	6344.866109	15.301799	-0.049369	4.304479
238.351067	6336.934725	15.306803	-0.049352	4.301882
238.222329	6328.901003	15.311808	-0.049323	4.299251
238.256845	6320.946395	15.316813	-0.049324	4.296644
238.382721	6312.944870	15.321818	-0.049343	4.294022
238.088054	6304.908154	15.326823	-0.049283	4.291383
238.169721	6296.880453	15.331827	-0.049293	4.288748
237.969367	6288.911289	15.336832	-0.049251	4.286129
237.890776	6280.891781	15.341837	-0.049231	4.283492
237.794545	6272.919454	15.346842	-0.049209	4.280870
237.757698	6264.941999	15.351847	-0.049197	4.278244
238.041326	6256.922319	15.356851	-0.049245	4.275606
237.990374	6248.895358	15.361856	-0.049230	4.272960
237.845182	6240.832323	15.366861	-0.049198	4.270301
237.946221	6232.890854	15.371866	-0.049212	4.267682
237.629828	6224.833923	15.376871	-0.049148	4.265019
237.540306	6216.950873	15.381875	-0.049127	4.262414
237.706491	6208.929800	15.386880	-0.049153	4.259765
237.757291	6200.918685	15.391885	-0.049157	4.257116
237.554665	6192.894966	15.396890	-0.049114	4.254459
237.475937	6184.824863	15.401895	-0.049095	4.251786
237.507088	6176.828406	15.406899	-0.049096	4.249136
237.305653	6168.876385	15.411904	-0.049053	4.246498
237.235238	6160.886193	15.416909	-0.049035	4.243846
237.186685	6152.944596	15.421914	-0.049021	4.241209
237.148594	6144.910892	15.426919	-0.049009	4.238540
237.037364	6136.942589	15.431923	-0.048984	4.235891
237.081217	6128.887567	15.436928	-0.048987	4.233212
237.052816	6120.862245	15.441933	-0.048976	4.230541
237.145551	6112.898435	15.446938	-0.048989	4.227890
237.094018	6104.887656	15.451943	-0.048974	4.225220
237.106991	6096.912811	15.456947	-0.048972	4.222561
236.845936	6088.921256	15.461952	-0.048918	4.219892
236.725912	6080.920341	15.466957	-0.048891	4.217219
236.855299	6072.926337	15.471962	-0.048910	4.214550
236.630576	6064.883733	15.476967	-0.048863	4.211859
236.805042	6056.891962	15.481971	-0.048891	4.209188
236.755831	6048.906515	15.486976	-0.048877	4.206514
236.671171	6040.906772	15.491981	-0.048856	4.203834
236.672487	6032.961634	15.496986	-0.048851	4.201171
236.274915	6024.924276	15.501991	-0.048772	4.198472
236.479269	6016.933651	15.506995	-0.048805	4.195792
236.472454	6008.841389	15.512000	-0.048799	4.193075
236.391871	6000.769751	15.517005	-0.048779	4.190362
236.255737	5992.843478	15.522010	-0.048749	4.187696
236.434994	5984.867559	15.527015	-0.048777	4.185014
236.334395	5976.938265	15.532019	-0.048754	4.182343
236.087361	5968.900303	15.537024	-0.048703	4.179633
236.366095	5960.879006	15.542029	-0.048750	4.176932
236.292714	5952.875410	15.547034	-0.048731	4.174232
236.149172	5944.827593	15.552039	-0.048699	4.171514
236.310226	5936.880195	15.557043	-0.048724	4.168831
236.167087	5928.874256	15.562048	-0.048693	4.166124
235.939361	5920.873693	15.567053	-0.048646	4.163415
235.960292	5912.930805	15.572058	-0.048645	4.160728
235.728957	5904.905869	15.577063	-0.048596	4.158007
235.723611	5896.872948	15.582067	-0.048591	4.155285
235.541529	5888.878136	15.587072	-0.048552	4.152572
235.723228	5880.803250	15.592077	-0.048581	4.149835
235.831137	5872.860312	15.597082	-0.048596	4.147139
235.574282	5864.821483	15.602087	-0.048543	4.144405
235.554033	5856.914611	15.607091	-0.048534	4.141717
235.723653	5848.870329	15.612096	-0.048561	4.138982
235.481113	5840.895612	15.617101	-0.048511	4.136264
235.479138	5832.872661	15.622106	-0.048505	4.133531
235.592391	5824.832529	15.627111	-0.048522	4.130792
235.318994	5816.863958	15.632115	-0.048466	4.128071
235.182407	5808.857337	15.637120	-0.048435	4.125336
235.104040	5800.878612	15.642125	-0.048416	4.122610
235.136049	5792.906590	15.647130	-0.048417	4.119886
235.265151	5784.866861	15.652135	-0.048436	4.117138
235.313251	5776.878350	15.657139	-0.048440	4.114404
235.333491	5768.803229	15.662144	-0.048439	4.111639
235.022495	5760.806185	15.667149	-0.048376	4.108895
235.028785	5752.861703	15.672154	-0.048372	4.106170
235.133438	5744.845976	15.677159	-0.048387	4.103421
235.043036	5736.877620	15.682163	-0.048365	4.100684
235.007341	5728.907974	15.687168	-0.048353	4.097945
235.062554	5720.915642	15.692173	-0.048359	4.095197
235.147279	5712.904829	15.697178	-0.048370	4.092442
234.803118	5704.854561	15.702183	-0.048300	4.089666
234.674247	5696.926430	15.707187	-0.048272	4.086933
234.815388	5688.882534	15.712192	-0.048293	4.084161
234.765646	5680.914060	15.717197	-0.048279	4.081411
234.502435	5672.939631	15.722202	-0.048225	4.078655
234.467405	5664.914566	15.727207	-0.048213	4.075882
234.687750	5656.883771	15.732211	-0.048249	4.073108
234.560577	5648.867045	15.737216	-0.048221	4.070333
234.286146	5640.887091	15.742221	-0.048165	4.067567
234.335251	5632.888626	15.747226	-0.048169	4.064797
234.195235	5624.925889	15.752231	-0.048138	4.062034
234.141925	5616.906570	15.757235	-0.048123	4.059252
234.195460	5608.952174	15.762240	-0.048128	4.056491
234.116827	5600.907168	15.767245	-0.048108	4.053695
234.183685	5592.926296	15.772250	-0.048116	4.050922
234.000103	5584.851060	15.777255	-0.048077	4.048110
234.215758	5576.880284	15.782259	-0.048112	4.045339
234.078321	5568.921831	15.787264	-0.048082	4.042565
233.796923	5560.889099	15.792269	-0.048024	4.039761
233.911371	5552.948878	15.797274	-0.048041	4.036993
233.857164	5544.901518	15.802279	-0.048025	4.034183
233.784296	5536.796273	15.807283	-0.048007	4.031351
233.855359	5528.803895	15.812288	-0.048015	4.028558
233.612609	5520.836984	15.817293	-0.047965	4.025768
233.707315	5512.901026	15.822298	-0.047978	4.022991
233.577110	5504.860139	15.827303	-0.047949	4.020173
233.696589	5496.942116	15.832307	-0.047966	4.017399
233.724991	5488.892986	15.837312	-0.047966	4.014576
233.556403	5480.860083	15.842317	-0.047930	4.011754
233.556199	5472.847575	15.847322	-0.047925	4.008939
233.462270	5464.868891	15.852327	-0.047902	4.006133
233.272527	5456.907273	15.857331	-0.047862	4.003330
233.319762	5448.911300	15.862336	-0.047866	4.000516
233.273470	5440.900397	15.867341	-0.047853	3.997693
233.185635	5432.909475	15.872346	-0.047831	3.994875
233.270067	5424.870308	15.877351	-0.047842	3.992041
233.384867	5416.867247	15.882355	-0.047858	3.989217
233.262112	5408.905563	15.887360	-0.047831	3.986403
233.070088	5400.876861	15.892365	-0.047790	3.983562
233.058717	5392.918750	15.897370	-0.047783	3.980746
232.890088	5384.904901	15.902375	-0.047747	3.977906
232.813246	5376.917191	15.907379	-0.047727	3.975075
232.993305	5368.854385	15.912384	-0.047756	3.972220
232.770381	5360.866604	15.917389	-0.047709	3.969382
232.887230	5352.936984	15.922394	-0.047726	3.966569
232.756141	5344.923810	15.927399	-0.047697	3.963720
232.792750	5336.939991	15.932403	-0.047699	3.960882
232.831434	5328.939855	15.937408	-0.047701	3.958036
232.637920	5320.954972	15.942413	-0.047660	3.955190
232.837206	5312.930521	15.947418	-0.047692	3.952334
232.800352	5304.887451	15.952423	-0.047680	3.949466
232.660572	5296.917395	15.957427	-0.047649	3.946619
232.679083	5288.932246	15.962432	-0.047648	3.943768
232.595516	5280.942198	15.967437	-0.047627	3.940912
232.623112	5272.973411	15.972442	-0.047628	3.938063
232.401073	5264.957424	15.977447	-0.047581	3.935190
232.320252	5256.946423	15.982451	-0.047561	3.932320
232.336393	5248.912058	15.987456	-0.047559	3.929441
232.024391	5240.962783	15.992461	-0.047496	3.926584
232.286960	5232.964255	15.997466	-0.047540	3.923718
232.215310	5224.967599	16.002471	-0.047522	3.920845
232.070339	5217.013576	16.007475	-0.047490	3.917983
232.228672	5208.960536	16.012480	-0.047515	3.915089
232.055825	5200.946884	16.017485	-0.047477	3.912201
232.055725	5192.934648	16.022490	-0.047473	3.909315
231.911092	5184.951404	16.027495	-0.047441	3.906434
231.949631	5176.932587	16.032499	-0.047443	3.903542
231.889955	5168.965455	16.037504	-0.047427	3.900665
231.740389	5160.976982	16.042509	-0.047394	3.897775
231.702939	5152.992061	16.047514	-0.047382	3.894888
231.590623	5144.952348	16.052519	-0.047356	3.891976
231.470640	5136.917388	16.057523	-0.047329	3.889064
231.475108	5128.969729	16.062528	-0.047325	3.886184
231.601407	5120.937135	16.067533	-0.047343	3.883274
231.725744	5112.963935	16.072538	-0.047362	3.880382
231.516909	5105.007655	16.077543	-0.047318	3.877489
231.607458	5096.979449	16.082547	-0.047330	3.874572
231.360022	5088.734460	16.087552	-0.047279	3.871568
231.351907	5080.796752	16.092557	-0.047272	3.868679
231.492153	5072.888595	16.097562	-0.047293	3.865800
231.443461	5064.867350	16.102567	-0.047279	3.862875
231.351517	5056.942684	16.107571	-0.047257	3.859982
231.263576	5048.959680	16.112576	-0.047236	3.857065
231.418506	5040.928339	16.117581	-0.047260	3.854134
231.517338	5032.951391	16.122586	-0.047273	3.851219
230.982518	5024.957726	16.127591	-0.047169	3.848283
230.946868	5016.937406	16.132595	-0.047157	3.845345
230.899944	5009.009866	16.137600	-0.047144	3.842438
230.809411	5000.996363	16.142605	-0.047122	3.839497
230.890767	4993.049909	16.147610	-0.047132	3.836581
230.797859	4985.019091	16.152615	-0.047110	3.833629
230.782352	4976.977376	16.157619	-0.047102	3.830672
230.920468	4968.974684	16.162624	-0.047123	3.827731
230.962851	4960.942886	16.167629	-0.047126	3.824774
230.820159	4953.033770	16.172634	-0.047094	3.821857
230.710183	4945.036637	16.177639	-0.047069	3.818905
230.864986	4937.033821	16.182643	-0.047093	3.815955
230.797950	4929.036477	16.187648	-0.047075	3.813000
230.503868	4921.012142	16.192653	-0.047016	3.810027
230.501949	4913.048012	16.197658	-0.047010	3.807081
230.515722	4905.016641	16.202663	-0.047008	3.804108
230.574234	4897.092522	16.207667	-0.047014	3.801173
230.496650	4889.062172	16.212672	-0.046994	3.798194
230.464274	4881.042216	16.217677	-0.046983	3.795217
230.405722	4873.030966	16.222682	-0.046968	3.792240
230.295926	4865.004738	16.227687	-0.046942	3.789255
230.091866	4857.016528	16.232691	-0.046899	3.786279
230.055421	4849.051475	16.237696	-0.046888	3.783313
229.979807	4841.034733	16.242701	-0.046869	3.780325
229.891352	4833.108843	16.247706	-0.046847	3.777368
229.771707	4825.052259	16.252711	-0.046820	3.774359
230.047930	4817.029944	16.257715	-0.046866	3.771369
229.904804	4809.042747	16.262720	-0.046835	3.768381
229.836031	4801.017364	16.267725	-0.046817	3.765377
229.934475	4793.084048	16.272730	-0.046830	3.762410
229.622843	4785.051374	16.277735	-0.046767	3.759393
229.625147	4777.100820	16.282739	-0.046763	3.756412
229.690383	4769.052057	16.287744	-0.046770	3.753394
229.561921	4761.036722	16.292749	-0.046741	3.750381
229.597254	4753.073329	16.297754	-0.046743	3.747389
229.631622	4744.966177	16.302759	-0.046744	3.744340
229.684214	4737.064264	16.307763	-0.046749	3.741367
229.473530	4729.097350	16.312768	-0.046705	3.738360
229.412053	4721.106022	16.317773	-0.046689	3.735345
229.499864	4713.134071	16.322778	-0.046700	3.732339
229.306617	4705.087996	16.327783	-0.046659	3.729296
229.111876	4697.132064	16.332787	-0.046618	3.726284
229.177441	4689.138829	16.337792	-0.046625	3.723262
229.197801	4681.134344	16.342797	-0.046624	3.720232
229.331889	4673.181792	16.347802	-0.046644	3.717222
229.247646	4665.130351	16.352807	-0.046623	3.714167
229.303511	4657.056798	16.357811	-0.046629	3.711104
229.283735	4649.074484	16.362816	-0.046620	3.708072
229.133852	4641.064476	16.367821	-0.046587	3.705023
229.166579	4633.156690	16.372826	-0.046589	3.702016
229.259636	4625.138278	16.377831	-0.046601	3.698965
229.165897	4617.150149	16.382835	-0.046579	3.695918
229.131507	4609.144298	16.387840	-0.046567	3.692864
228.810661	4601.139445	16.392845	-0.046503	3.689800
228.691752	4593.186853	16.397850	-0.046476	3.686759
228.719972	4585.182156	16.402855	-0.046476	3.683699
228.763819	4577.188771	16.407859	-0.046479	3.680642
228.718453	4569.227521	16.412864	-0.046466	3.677591
228.737857	4561.204251	16.417869	-0.046464	3.674517
228.785325	4553.179304	16.422874	-0.046468	3.671439
228.632413	4545.173736	16.427879	-0.046435	3.668362
228.609973	4537.166970	16.432883	-0.046426	3.665284
228.683045	4529.199430	16.437888	-0.046434	3.662222
228.457808	4521.191475	16.442893	-0.046387	3.659134
228.438088	4513.253358	16.447898	-0.046379	3.656075
228.279519	4505.217251	16.452903	-0.046344	3.652972
228.393986	4497.166939	16.457907	-0.046361	3.649869
228.455699	4489.196535	16.462912	-0.046367	3.646792
228.371561	4481.204929	16.467917	-0.046347	3.643701
228.285593	4473.242052	16.472922	-0.046326	3.640618
228.237962	4465.254298	16.477927	-0.046312	3.637523
228.208390	4457.234268	16.482931	-0.046301	3.634414
228.286416	4449.191104	16.487936	-0.046311	3.631297
228.032129	4441.182025	16.492941	-0.046259	3.628181
227.889835	4433.204236	16.497946	-0.046227	3.625077
227.807882	4425.239546	16.502951	-0.046207	3.621978
227.855625	4417.255753	16.507955	-0.046211	3.618872
227.671619	4409.301558	16.512960	-0.046172	3.615768
227.573301	4401.236962	16.517965	-0.046149	3.612621
227.699026	4393.256314	16.522970	-0.046167	3.609510
227.506638	4385.309118	16.527975	-0.046126	3.606401
227.488764	4377.292554	16.532979	-0.046118	3.603267
227.488920	4369.311998	16.537984	-0.046113	3.600145
227.341707	4361.332203	16.542989	-0.046081	3.597016
227.418207	4353.321043	16.547994	-0.046090	3.593878
227.257137	4345.310907	16.552999	-0.046055	3.590731
227.283367	4337.313406	16.558003	-0.046055	3.587592
227.223576	4329.304515	16.563008	-0.046039	3.584443
227.128523	4321.347309	16.568013	-0.046016	3.581311
227.145020	4313.361237	16.573018	-0.046015	3.578168
227.158475	4305.345969	16.578023	-0.046012	3.575010
227.098007	4297.358232	16.583027	-0.045996	3.571859
227.040820	4289.353617	16.588032	-0.045980	3.568698
226.958563	4281.348493	16.593037	-0.045960	3.565533
226.991156	4273.389392	16.598042	-0.045961	3.562387
226.657109	4265.376139	16.603047	-0.045894	3.559206
226.767742	4257.418346	16.608051	-0.045910	3.556057
226.655664	4249.333003	16.613056	-0.045884	3.552848
226.530772	4241.270919	16.618061	-0.045856	3.549645
226.694417	4233.347013	16.623066	-0.045881	3.546503
226.610513	4225.355997	16.628071	-0.045861	3.543324
226.512611	4217.352072	16.633075	-0.045837	3.540136
226.464085	4209.380676	16.638080	-0.045824	3.536960
226.439824	4201.355134	16.643085	-0.045814	3.533760
226.371052	4193.389526	16.648090	-0.045796	3.530580
226.109377	4185.417652	16.653095	-0.045743	3.527389
226.278453	4177.386740	16.658099	-0.045769	3.524184
226.336776	4169.456540	16.663104	-0.045775	3.521014
226.047653	4161.452509	16.668109	-0.045716	3.517800
225.989971	4153.477099	16.673114	-0.045701	3.514602
225.941655	4145.453029	16.678119	-0.045687	3.511381
226.004649	4137.408332	16.683123	-0.045693	3.508153
226.035372	4129.437182	16.688128	-0.045694	3.504951
225.874719	4121.464868	16.693133	-0.045659	3.501739
226.079877	4113.491673	16.698138	-0.045693	3.498535
225.907911	4105.488477	16.703143	-0.045656	3.495304
225.938881	4097.483879	16.708147	-0.045657	3.492076
225.888462	4089.499227	16.713152	-0.045642	3.488851
225.601657	4081.514284	16.718157	-0.045584	3.485615
225.667816	4073.560811	16.723162	-0.045591	3.482400
225.848890	4065.507711	16.728167	-0.045620	3.479145
225.592094	4057.571376	16.733171	-0.045567	3.475921
225.650026	4049.536040	16.738176	-0.045573	3.472664
225.664840	4041.491663	16.743181	-0.045571	3.469398
225.743476	4033.528865	16.748186	-0.045581	3.466164
225.405390	4025.546896	16.753191	-0.045513	3.462907
225.285885	4017.584996	16.758195	-0.045486	3.459661
225.285982	4009.598829	16.763200	-0.045481	3.456406
225.223872	4001.556344	16.768205	-0.045464	3.453124
225.346970	3993.570042	16.773210	-0.045482	3.449867
225.326346	3985.560849	16.778215	-0.045473	3.446593
225.182498	3977.592907	16.783219	-0.045442	3.443328
225.094029	3969.603710	16.788224	-0.045420	3.440054
224.951801	3961.651663	16.793229	-0.045389	3.436790
224.998450	3953.636310	16.798234	-0.045393	3.433503
224.966423	3945.584137	16.803239	-0.045382	3.430195
225.040764	3937.591004	16.808243	-0.045391	3.426912
225.097971	3929.612975	16.813248	-0.045396	3.423632
224.824670	3921.631902	16.818253	-0.045340	3.420335
224.760963	3913.701154	16.823258	-0.045324	3.417064
224.790396	3905.656896	16.828263	-0.045324	3.413745
224.853158	3897.641107	16.833267	-0.045331	3.410437
224.659875	3889.695109	16.838272	-0.045290	3.407145
224.649878	3881.651134	16.843277	-0.045283	3.403816
224.772391	3873.712445	16.848282	-0.045301	3.400531
224.771815	3865.723945	16.853287	-0.045296	3.397219
224.628588	3857.728141	16.858291	-0.045264	3.393895
224.671926	3849.670478	16.863296	-0.045268	3.390549
224.424087	3841.682809	16.868301	-0.045216	3.387218
224.431475	3833.709293	16.873306	-0.045213	3.383899
224.400821	3825.736336	16.878311	-0.045202	3.380576
224.379089	3817.774221	16.883315	-0.045193	3.377254
224.238621	3809.776242	16.888320	-0.045162	3.373910
224.098274	3801.736229	16.893325	-0.045131	3.370545
224.162658	3793.780805	16.898330	-0.045138	3.367219
223.981360	3785.778993	16.903335	-0.045099	3.363861
224.055618	3777.787147	16.908339	-0.045108	3.360514
224.139862	3769.823940	16.913344	-0.045119	3.357176
224.009623	3761.792758	16.918349	-0.045090	3.353798
224.023571	3753.801063	16.923354	-0.045088	3.350438
223.919189	3745.807610	16.928359	-0.045063	3.347070
223.782912	3737.802063	16.933363	-0.045033	3.343692
223.732543	3729.855654	16.938368	-0.045019	3.340339
223.494254	3721.871544	16.943373	-0.044969	3.336960
223.696189	3713.846100	16.948378	-0.045002	3.333576
223.605465	3705.849913	16.953383	-0.044980	3.330190
223.494587	3697.878411	16.958387	-0.044954	3.326811
223.621686	3689.894137	16.963392	-0.044973	3.323431
223.273041	3681.920147	16.968397	-0.044903	3.320035
223.289856	3673.955264	16.973402	-0.044902	3.316652
223.328130	3665.922478	16.978407	-0.044904	3.313238
223.378544	3657.886615	16.983411	-0.044908	3.309820
223.264871	3649.935143	16.988416	-0.044882	3.306428
223.095799	3641.943416	16.993421	-0.044846	3.303013
223.132915	3633.964283	16.998426	-0.044848	3.299608
223.082625	3626.002654	17.003431	-0.044833	3.296204
222.975893	3617.984323	17.008435	-0.044809	3.292769
223.143466	3609.963601	17.013440	-0.044835	3.289340
222.979330	3601.998510	17.018445	-0.044799	3.285919
223.115099	3594.014725	17.023450	-0.044820	3.282498
222.992380	3586.035711	17.028455	-0.044792	3.279066
223.043889	3578.053674	17.033459	-0.044797	3.275635
222.942735	3570.058331	17.038464	-0.044773	3.272189
222.881352	3562.025125	17.043469	-0.044756	3.268724
222.881498	3554.054886	17.048474	-0.044751	3.265286
222.829700	3546.067449	17.053479	-0.044737	3.261834
222.604816	3538.100745	17.058483	-0.044690	3.258381
222.569029	3530.112259	17.063488	-0.044678	3.254922
222.742693	3522.050360	17.068493	-0.044706	3.251436
222.726067	3514.096583	17.073498	-0.044698	3.247985
222.429423	3506.123241	17.078503	-0.044638	3.244512
222.437483	3498.159807	17.083507	-0.044634	3.241051
222.441327	3490.180889	17.088512	-0.044630	3.237579
222.362794	3482.152287	17.093517	-0.044610	3.234079
222.504871	3474.110434	17.098522	-0.044632	3.230577
222.194994	3466.145157	17.103527	-0.044569	3.227088
222.132517	3458.147656	17.108531	-0.044553	3.223590
222.268623	3450.172348	17.113536	-0.044573	3.220107
222.252138	3442.200704	17.118541	-0.044565	3.216615
222.108591	3434.243994	17.123546	-0.044534	3.213120
222.016013	3426.208742	17.128551	-0.044511	3.209590
221.936419	3418.213817	17.133555	-0.044492	3.206073
221.830085	3410.276344	17.138560	-0.044467	3.202577
221.567875	3402.300033	17.143565	-0.044413	3.199054
221.599767	3394.316706	17.148570	-0.044414	3.195536
221.750213	3386.271475	17.153575	-0.044437	3.191991
221.734556	3378.272861	17.158579	-0.044429	3.188456
221.546062	3370.306011	17.163584	-0.044389	3.184924
221.590118	3362.320163	17.168589	-0.044393	3.181390
221.751753	3354.341730	17.173594	-0.044418	3.177860
221.628539	3346.346772	17.178599	-0.044390	3.174307
221.624265	3338.336719	17.183603	-0.044384	3.170747
221.714052	3330.369364	17.188608	-0.044396	3.167207
221.450239	3322.394665	17.193613	-0.044342	3.163645
221.380428	3314.426356	17.198618	-0.044324	3.160090
221.523414	3306.431683	17.203623	-0.044346	3.156528
221.288851	3298.431067	17.208627	-0.044297	3.152943
221.334185	3290.409561	17.213632	-0.044300	3.149356
221.234107	3282.398851	17.218637	-0.044277	3.145765
221.410864	3274.441200	17.223642	-0.044305	3.142205
221.161102	3266.486394	17.228647	-0.044253	3.138623
221.039107	3258.494897	17.233651	-0.044226	3.135026
221.091196	3250.504491	17.238656	-0.044231	3.131434
220.878764	3242.498092	17.243661	-0.044186	3.127818
220.981665	3234.511371	17.248666	-0.044200	3.124221
220.911807	3226.564060	17.253671	-0.044182	3.120631
220.965436	3218.560509	17.258675	-0.044187	3.117016
220.725053	3210.605825	17.263680	-0.044138	3.113405
220.790489	3202.544590	17.268685	-0.044145	3.109756
220.878026	3194.591013	17.273690	-0.044156	3.106153
220.759176	3186.606820	17.278695	-0.044129	3.102522
220.549519	3178.645947	17.283699	-0.044085	3.098893
220.462501	3170.683552	17.288704	-0.044064	3.095265
220.312898	3162.645775	17.293709	-0.044031	3.091596
220.403348	3154.646060	17.298714	-0.044043	3.087950
220.371542	3146.665374	17.303719	-0.044032	3.084303
220.252885	3138.700892	17.308723	-0.044005	3.080655
220.278677	3130.746242	17.313728	-0.044005	3.077015
220.026992	3122.719619	17.318733	-0.043953	3.073323
220.236728	3114.643535	17.323738	-0.043987	3.069627
220.072638	3106.672937	17.328743	-0.043952	3.065956
220.007741	3098.707931	17.333747	-0.043935	3.062289
220.008375	3090.755272	17.338752	-0.043930	3.058626
219.946906	3082.791451	17.343757	-0.043914	3.054950
219.962718	3074.776594	17.348762	-0.043912	3.051251
219.828944	3066.804408	17.353767	-0.043882	3.047559
219.595909	3058.846130	17.358771	-0.043834	3.043864
219.719283	3050.848664	17.363776	-0.043852	3.040164
219.717428	3042.881242	17.368781	-0.043846	3.036467
219.821338	3034.875608	17.373786	-0.043861	3.032753
219.583607	3026.881710	17.378791	-0.043812	3.029024
219.368581	3018.912836	17.383795	-0.043767	3.025302
219.478198	3010.953456	17.388800	-0.043782	3.021597
219.412908	3002.958581	17.393805	-0.043765	3.017861
219.403771	2994.975768	17.398810	-0.043758	3.014129
219.205670	2986.969343	17.403815	-0.043717	3.010373
219.120101	2979.019779	17.408819	-0.043696	3.006643
219.248206	2971.040327	17.413824	-0.043715	3.002906
219.069152	2963.033415	17.418829	-0.043676	2.999136
219.108451	2955.074611	17.423834	-0.043679	2.995395
218.934202	2947.049633	17.428839	-0.043641	2.991607
218.984883	2939.034865	17.433843	-0.043646	2.987830
219.149497	2931.051137	17.438848	-0.043672	2.984069
218.790124	2923.110747	17.443853	-0.043600	2.980297
218.777784	2915.152144	17.448858	-0.043593	2.976530
218.841901	2907.123697	17.453863	-0.043599	2.972728
218.913643	2899.117163	17.458867	-0.043608	2.968932
218.679263	2891.183870	17.463872	-0.043559	2.965151
218.622661	2883.214174	17.468877	-0.043544	2.961356
218.542190	2875.237644	17.473882	-0.043524	2.957552
218.440362	2867.240363	17.478887	-0.043500	2.953733
218.342628	2859.233440	17.483891	-0.043477	2.949904
218.558542	2851.248691	17.488896	-0.043512	2.946096
218.484339	2843.270419	17.493901	-0.043493	2.942272
218.422261	2835.308399	17.498906	-0.043477	2.938451
218.343951	2827.320842	17.503911	-0.043457	2.934613
218.218800	2819.340447	17.508915	-0.043429	2.930770
218.235429	2811.353808	17.513920	-0.043427	2.926926
218.173480	2803.384951	17.518925	-0.043411	2.923082
218.259918	2795.401301	17.523930	-0.043422	2.919234
217.968463	2787.472194	17.528935	-0.043363	2.915386
217.975040	2779.363623	17.533939	-0.043359	2.911463
217.917130	2771.393484	17.538944	-0.043343	2.907598
217.863499	2763.428357	17.543949	-0.043329	2.903730
217.587033	2755.476026	17.548954	-0.043272	2.899852
217.584904	2747.519495	17.553959	-0.043267	2.895981
217.612246	2739.496046	17.558963	-0.043267	2.892074
217.737148	2731.510957	17.563968	-0.043285	2.888185
217.337267	2723.571974	17.568973	-0.043206	2.884286
217.340334	2715.613045	17.573978	-0.043202	2.880393
217.381031	2707.621179	17.578983	-0.043204	2.876481
217.382091	2699.607068	17.583987	-0.043199	2.872550
217.448167	2691.602356	17.588992	-0.043207	2.868622
217.450502	2683.605577	17.593997	-0.043202	2.864689
217.371794	2675.701743	17.599002	-0.043183	2.860792
217.348373	2667.705701	17.604007	-0.043173	2.856848
217.273756	2659.725861	17.609011	-0.043155	2.852903
217.272009	2651.750122	17.614016	-0.043149	2.848959
217.034363	2643.769303	17.619021	-0.043100	2.844993
217.288510	2635.781701	17.624026	-0.043143	2.841046
216.945119	2627.855992	17.629031	-0.043074	2.837091
216.941597	2619.833204	17.634035	-0.043068	2.833101
216.972883	2611.843434	17.639040	-0.043069	2.829124
216.742113	2603.844138	17.644045	-0.043021	2.825121
216.804419	2595.891492	17.649050	-0.043028	2.821153
216.725620	2587.916263	17.654055	-0.043008	2.817160
216.782972	2579.919315	17.659059	-0.043014	2.813159
216.761017	2571.945942	17.664064	-0.043005	2.809158
216.633265	2563.937733	17.669069	-0.042976	2.805129
216.641738	2556.006018	17.674074	-0.042973	2.801140
216.731368	2548.045869	17.679079	-0.042985	2.797135
216.457534	2540.052550	17.684083	-0.042929	2.793087
216.496784	2532.062461	17.689088	-0.042931	2.789054
216.435161	2524.067873	17.694093	-0.042915	2.785006
216.373547	2516.123118	17.699098	-0.042898	2.780977
216.119632	2508.179725	17.704103	-0.042846	2.776932
216.171000	2500.163298	17.709107	-0.042851	2.772862
216.197190	2492.184852	17.714112	-0.042851	2.768803
215.938565	2484.202462	17.719117	-0.042798	2.764720
215.917615	2476.271370	17.724122	-0.042789	2.760671
215.886582	2468.294513	17.729127	-0.042778	2.756592
215.783241	2460.250225	17.734131	-0.042754	2.752468
216.011705	2452.220320	17.739136	-0.042791	2.748366
215.793736	2444.268955	17.744141	-0.042746	2.744270
215.812433	2436.320403	17.749146	-0.042744	2.740185
215.645125	2428.363317	17.754151	-0.042708	2.736077
215.794938	2420.349194	17.759155	-0.042731	2.731953
215.652749	2412.416211	17.764160	-0.042700	2.727847
215.471766	2404.429307	17.769165	-0.042661	2.723704
215.496915	2396.471027	17.774170	-0.042661	2.719583
215.425358	2388.530328	17.779175	-0.042643	2.715459
215.446238	2380.504229	17.784179	-0.042642	2.711289
215.308065	2372.531693	17.789184	-0.042611	2.707131
215.093087	2364.586681	17.794189	-0.042566	2.702976
215.164998	2356.614149	17.799194	-0.042575	2.698819
215.312950	2348.622629	17.804199	-0.042597	2.694650
215.203481	2340.630344	17.809203	-0.042572	2.690458
215.112530	2332.698894	17.814208	-0.042550	2.686292
215.024793	2324.702801	17.819213	-0.042529	2.682086
215.031933	2316.777768	17.824218	-0.042525	2.677917
214.937198	2308.782120	17.829223	-0.042503	2.673697
214.733519	2300.767465	17.834227	-0.042460	2.669454
214.851530	2292.782570	17.839232	-0.042477	2.665241
214.750450	2284.841066	17.844237	-0.042453	2.661030
214.517179	2276.897740	17.849242	-0.042405	2.656802
214.501480	2268.903580	17.854247	-0.042397	2.652555
214.578369	2260.886262	17.859251	-0.042406	2.648295
214.540396	2252.945939	17.864256	-0.042394	2.644061
214.280434	2245.001210	17.869261	-0.042341	2.639804
214.305810	2237.030535	17.874266	-0.042341	2.635544
214.499264	2229.010647	17.879271	-0.042372	2.631263
214.394352	2221.041110	17.884275	-0.042347	2.626982
214.257031	2213.101985	17.889280	-0.042317	2.622708
214.187483	2205.118498	17.894285	-0.042299	2.618407
214.182593	2197.165030	17.899290	-0.042293	2.614120
213.906271	2189.193899	17.904295	-0.042237	2.609798
214.002611	2181.210243	17.909299	-0.042250	2.605488
214.197196	2173.241606	17.914304	-0.042281	2.601185
214.118265	2165.289123	17.919309	-0.042262	2.596865
214.103125	2157.217675	17.924314	-0.042254	2.592477
214.062627	2149.153041	17.929319	-0.042241	2.588084
213.581432	2141.264630	17.934323	-0.042147	2.583750
213.636508	2133.326679	17.939328	-0.042152	2.579418
213.663022	2125.367704	17.944333	-0.042152	2.575065
213.762523	2117.379394	17.949338	-0.042166	2.570694
213.483681	2109.454606	17.954343	-0.042109	2.566324
213.360035	2101.515646	17.959347	-0.042081	2.561949
213.721754	2093.527483	17.964352	-0.042143	2.557574
213.372848	2085.582905	17.969357	-0.042074	2.553165
213.349542	2077.591460	17.974362	-0.042064	2.548746
213.257629	2069.643165	17.979367	-0.042042	2.544338
213.327628	2061.670367	17.984371	-0.042050	2.539921
213.121978	2053.747378	17.989376	-0.042007	2.535504
213.032625	2045.741373	17.994381	-0.041986	2.531041
213.048231	2037.770235	17.999386	-0.041984	2.526597
213.046605	2029.812241	18.004391	-0.041978	2.522151
213.077227	2021.854660	18.009395	-0.041979	2.517700
213.086771	2013.886569	18.014400	-0.041976	2.513234
212.746786	2005.908172	18.019405	-0.041908	2.508729
212.872157	1997.916228	18.024410	-0.041926	2.504242
212.800919	1989.981604	18.029415	-0.041908	2.499764
212.728937	1982.019897	18.034419	-0.041890	2.495264
212.617936	1974.061099	18.039424	-0.041864	2.490754
212.573449	1966.088066	18.044429	-0.041851	2.486232
212.593829	1958.137619	18.049434	-0.041850	2.481720
212.537872	1950.186034	18.054439	-0.041834	2.477194
212.386639	1942.209685	18.059443	-0.041801	2.472637
212.440962	1934.224601	18.064448	-0.041806	2.468083
212.514857	1926.239113	18.069453	-0.041815	2.463522
212.178298	1918.337552	18.074458	-0.041748	2.458969
212.178906	1910.384935	18.079463	-0.041743	2.454404
212.165825	1902.376227	18.084467	-0.041736	2.449798
212.151694	1894.428192	18.089472	-0.041728	2.445217
212.003099	1886.484102	18.094477	-0.041695	2.440620
212.016018	1878.531901	18.099482	-0.041693	2.436022
212.041298	1870.484070	18.104487	-0.041693	2.431360
211.834545	1862.524476	18.109491	-0.041649	2.426723
212.153103	1854.547174	18.114496	-0.041704	2.422107
211.858739	1846.633436	18.119501	-0.041644	2.417473
211.901637	1838.671871	18.124506	-0.041647	2.412827
211.745967	1830.713074	18.129511	-0.041613	2.408159
211.714722	1822.744462	18.134515	-0.041602	2.403485
211.629421	1814.830425	18.139520	-0.041582	2.398830
211.591078	1806.853712	18.144525	-0.041570	2.394133
211.766264	1798.865980	18.149530	-0.041597	2.389437
211.629757	1790.926309	18.154535	-0.041567	2.384736
211.229506	1783.003215	18.159539	-0.041487	2.380014
211.449923	1775.034339	18.164544	-0.041524	2.375305
211.554507	1767.038171	18.169549	-0.041538	2.370561
211.312643	1759.110067	18.174554	-0.041488	2.365821
211.271972	1751.184468	18.179559	-0.041476	2.361088
211.175725	1743.231941	18.184563	-0.041453	2.356326
211.312125	1735.210214	18.189568	-0.041473	2.351531
211.068707	1727.254352	18.194573	-0.041423	2.346735
211.043971	1719.327247	18.199578	-0.041414	2.341964
211.070450	1711.370802	18.204583	-0.041414	2.337170
210.868026	1703.416598	18.209587	-0.041371	2.332349
210.906163	1695.452908	18.214592	-0.041373	2.327531
210.827396	1687.506183	18.219597	-0.041354	2.322705
210.812491	1679.569605	18.224602	-0.041346	2.317879
210.935336	1671.595643	18.229607	-0.041364	2.313033
210.822022	1663.638956	18.234611	-0.041338	2.308167
210.625571	1655.715100	18.239616	-0.041296	2.303304
210.552701	1647.767470	18.244621	-0.041278	2.298426
210.649298	1639.800500	18.249626	-0.041291	2.293540
210.538563	1631.847818	18.254631	-0.041265	2.288636
210.305438	1623.900307	18.259635	-0.041217	2.283713
210.595858	1615.945962	18.264640	-0.041266	2.278820
210.484381	1607.988304	18.269645	-0.041241	2.273880
210.346100	1599.971855	18.274650	-0.041210	2.268891
210.330791	1592.030739	18.279655	-0.041202	2.263948
210.301998	1584.095084	18.284659	-0.041192	2.258997
210.157644	1576.196892	18.289664	-0.041160	2.254048
209.958639	1568.223922	18.294669	-0.041118	2.249036
209.757829	1560.287726	18.299674	-0.041076	2.244036
209.747934	1552.357061	18.304679	-0.041069	2.239045
209.546985	1544.423059	18.309683	-0.041027	2.234024
209.774785	1536.425532	18.314688	-0.041064	2.228990
209.766297	1528.474594	18.319693	-0.041058	2.223952
209.382496	1520.582068	18.324698	-0.040981	2.218907
209.622421	1512.600956	18.329703	-0.041021	2.213850
209.399188	1504.656645	18.334707	-0.040975	2.208763
209.277781	1496.729106	18.339712	-0.040947	2.203684
209.156211	1488.803146	18.344717	-0.040920	2.198594
209.332117	1480.826859	18.349722	-0.040947	2.193488
209.360065	1472.847319	18.354727	-0.040948	2.188353
209.074586	1464.932581	18.359731	-0.040890	2.183220
209.057470	1456.999041	18.364736	-0.040882	2.178087
209.127478	1449.038629	18.369741	-0.040890	2.172933
209.011976	1441.097044	18.374746	-0.040863	2.167761
208.795161	1433.193938	18.379751	-0.040818	2.162593
208.754075	1425.252556	18.384755	-0.040806	2.157404
209.071265	1417.261954	18.389760	-0.040860	2.152203
208.748814	1409.356504	18.394765	-0.040795	2.146986
208.584945	1401.438761	18.399770	-0.040759	2.141762
208.604147	1393.491944	18.404775	-0.040758	2.136524
208.361817	1385.562052	18.409779	-0.040708	2.131260
208.472365	1377.602332	18.414784	-0.040724	2.125996
208.517351	1369.657582	18.419789	-0.040727	2.120723
208.432447	1361.753847	18.424794	-0.040706	2.115452
208.194585	1353.771443	18.429799	-0.040657	2.110100
208.188041	1345.807443	18.434803	-0.040651	2.104769
208.375540	1337.872217	18.439808	-0.040681	2.099463
208.292486	1329.944899	18.444813	-0.040661	2.094122
208.082405	1322.022999	18.449818	-0.040617	2.088759
208.127028	1314.088704	18.454823	-0.040620	2.083399
207.862736	1306.198352	18.459827	-0.040566	2.078024
207.826543	1298.273556	18.464832	-0.040554	2.072634
207.873661	1290.299796	18.469837	-0.040558	2.067205
207.883468	1282.368803	18.474842	-0.040555	2.061788
207.583375	1274.486449	18.479847	-0.040494	2.056358
207.605734	1266.528169	18.484851	-0.040494	2.050894
207.817656	1258.561207	18.489856	-0.040528	2.045429
207.501166	1250.681460	18.494861	-0.040464	2.039956
207.537916	1242.765944	18.499866	-0.040466	2.034479
207.267041	1234.832795	18.504871	-0.040411	2.028944
207.257295	1226.881852	18.509875	-0.040404	2.023408
207.234491	1218.975346	18.514880	-0.040395	2.017886
207.149233	1211.030449	18.519885	-0.040374	2.012316
207.241996	1203.077237	18.524890	-0.040387	2.006743
207.140225	1195.183271	18.529895	-0.040363	2.001176
207.196033	1187.256795	18.534899	-0.040368	1.995587
207.249634	1179.317326	18.539904	-0.040373	1.989973
206.817932	1171.439035	18.544909	-0.040288	1.984335
206.720331	1163.529069	18.549914	-0.040265	1.978694
206.872336	1155.581107	18.554919	-0.040289	1.973036
206.800778	1147.647822	18.559923	-0.040270	1.967349
206.795250	1139.753029	18.564928	-0.040264	1.961679
206.659495	1131.841879	18.569933	-0.040234	1.955968
206.695954	1123.870899	18.574938	-0.040236	1.950215
206.600689	1115.959726	18.579943	-0.040214	1.944474
206.552332	1108.040882	18.584947	-0.040200	1.938716
206.627125	1100.116767	18.589952	-0.040209	1.932950
206.430700	1092.204194	18.594957	-0.040167	1.927145
206.301148	1084.317192	18.599962	-0.040138	1.921349
206.278098	1076.409566	18.604967	-0.040129	1.915532
206.246943	1068.474974	18.609971	-0.040118	1.909677
206.293179	1060.562677	18.614976	-0.040122	1.903829
206.054890	1052.672201	18.619981	-0.040073	1.897946
206.093488	1044.756136	18.624986	-0.040075	1.892058
205.884567	1036.865758	18.629991	-0.040031	1.886143
205.766236	1028.961308	18.634995	-0.040004	1.880208
205.833441	1021.064794	18.640000	-0.040012	1.874282
205.600240	1013.138950	18.645005	-0.039964	1.868280
205.584680	1005.228555	18.650010	-0.039956	1.862296
205.627391	997.323963	18.655015	-0.039959	1.856304
205.556209	989.399412	18.660019	-0.039941	1.850264
205.387225	981.528211	18.665024	-0.039905	1.844233
205.422489	973.610610	18.670029	-0.039906	1.838171
205.438150	965.706053	18.675034	-0.039904	1.832097
205.343867	957.809831	18.680039	-0.039882	1.825996
205.227287	949.925558	18.685043	-0.039855	1.819881
205.364755	942.021606	18.690048	-0.039876	1.813760
205.096531	934.132060	18.695053	-0.039821	1.807581
204.887631	926.265493	18.700058	-0.039777	1.801406
204.981804	918.369753	18.705063	-0.039790	1.795224
205.004196	910.394628	18.710067	-0.039789	1.788949
204.870466	902.526110	18.715072	-0.039760	1.782717
204.447863	894.694328	18.720077	-0.039676	1.776457
204.473077	886.769849	18.725082	-0.039676	1.770156
204.662262	878.854392	18.730087	-0.039706	1.763860
204.366780	871.013056	18.735091	-0.039646	1.757540
204.411733	863.122924	18.740096	-0.039650	1.751201
204.342074	855.223404	18.745101	-0.039632	1.744817
204.390587	847.341607	18.750106	-0.039636	1.738439
204.339081	839.461778	18.755111	-0.039622	1.732026
204.128446	831.589337	18.760115	-0.039578	1.725575
203.932534	823.758436	18.765120	-0.039536	1.719136
203.880071	815.867536	18.770125	-0.039522	1.712642
203.782126	807.973331	18.775130	-0.039498	1.706114
203.863263	800.081872	18.780135	-0.039509	1.699587
203.736719	792.214998	18.785139	-0.039480	1.693028
203.540357	784.362850	18.790144	-0.039439	1.686446
203.660783	776.458983	18.795149	-0.039456	1.679837
203.490344	768.629194	18.800154	-0.039420	1.673226
203.457660	760.749769	18.805159	-0.039409	1.666565
203.243191	752.894895	18.810163	-0.039364	1.659873
203.396150	745.015031	18.815168	-0.039388	1.653183
203.286650	737.140160	18.820173	-0.039362	1.646434
203.170760	729.309166	18.825178	-0.039336	1.639694
203.139643	721.446115	18.830183	-0.039325	1.632911
202.854545	713.560955	18.835187	-0.039267	1.626044
202.876152	705.701800	18.840192	-0.039267	1.619214
202.819508	697.841514	18.845197	-0.039251	1.612343
202.750949	689.983416	18.850202	-0.039234	1.605443
202.829848	682.143727	18.855207	-0.039243	1.598550
202.801403	674.280644	18.860211	-0.039233	1.591591
202.469102	666.487332	18.865216	-0.039167	1.584620
202.361892	658.650243	18.870221	-0.039142	1.577612
202.511756	650.763953	18.875226	-0.039165	1.570565
202.519986	642.931719	18.880231	-0.039162	1.563515
202.126557	635.151484	18.885235	-0.039084	1.556421
202.048104	627.298466	18.890240	-0.039064	1.549275
202.126583	619.429280	18.895245	-0.039074	1.542104
201.958814	611.619008	18.900250	-0.039038	1.534916
202.101397	603.754242	18.905255	-0.039059	1.527692
201.801494	595.963611	18.910259	-0.038999	1.520435
201.991888	588.125364	18.915264	-0.039029	1.513173
201.707889	580.315504	18.920269	-0.038972	1.505830
201.670266	572.503579	18.925274	-0.038960	1.498487
201.602720	564.685458	18.930279	-0.038942	1.491097
201.412432	556.890543	18.935283	-0.038902	1.483674
201.514680	549.071808	18.940288	-0.038916	1.476236
201.424179	541.210125	18.945293	-0.038895	1.468689
201.092658	533.440889	18.950298	-0.038828	1.461154
201.191533	525.623731	18.955303	-0.038842	1.453602
200.860130	517.846927	18.960307	-0.038775	1.445980
201.019733	510.033688	18.965312	-0.038800	1.438362
200.887214	502.249422	18.970317	-0.038771	1.430684
200.751755	494.463240	18.975322	-0.038741	1.422963
200.906912	486.655189	18.980327	-0.038765	1.415225
200.591487	478.897982	18.985331	-0.038701	1.407418
200.590666	471.125300	18.990336	-0.038696	1.399604
200.620155	463.330822	18.995341	-0.038697	1.391730
200.462930	455.554356	19.000346	-0.038663	1.383797
200.288382	447.813416	19.005351	-0.038626	1.375851
200.144489	440.041667	19.010355	-0.038594	1.367834
200.030286	432.297656	19.015360	-0.038568	1.359802
199.924711	424.543837	19.020365	-0.038544	1.351714
199.915262	416.770127	19.025370	-0.038537	1.343574
199.900539	409.021010	19.030375	-0.038529	1.335408
199.726451	401.271912	19.035379	-0.038492	1.327165
199.587157	393.559750	19.040384	-0.038462	1.318915
199.406086	385.755149	19.045389	-0.038423	1.310506
199.408336	377.958343	19.050394	-0.038419	1.302085
199.233878	370.266498	19.055399	-0.038381	1.293691
199.325218	362.502633	19.060403	-0.038394	1.285212
199.225718	354.820872	19.065408	-0.038370	1.276732
199.062121	347.117317	19.070413	-0.038335	1.268159
198.951780	339.418883	19.075418	-0.038310	1.259543
199.085962	331.690376	19.080423	-0.038330	1.250881
198.791220	324.030593	19.085427	-0.038270	1.242154
198.604715	316.374835	19.090432	-0.038231	1.233391
198.609267	308.646472	19.095437	-0.038227	1.224518
198.546683	300.967624	19.100442	-0.038211	1.215625
198.626796	293.271466	19.105447	-0.038221	1.206675
198.211685	285.668198	19.110451	-0.038139	1.197667
198.382303	277.967614	19.115456	-0.038166	1.188595
198.207216	270.331897	19.120461	-0.038129	1.179459
198.018586	262.703205	19.125466	-0.038089	1.170258
198.103436	255.045899	19.130471	-0.038100	1.161006
197.932720	247.411370	19.135475	-0.038063	1.151654
197.879073	239.761531	19.140480	-0.038049	1.142231
197.769098	232.149405	19.145485	-0.038024	1.132765
197.541061	224.563386	19.150490	-0.037976	1.123226
197.629549	216.940843	19.155495	-0.037988	1.113628
197.458368	209.356859	19.160499	-0.037952	1.103939
197.416234	201.782083	19.165504	-0.037939	1.094205
197.254144	194.213238	19.170509	-0.037904	1.084363
197.195280	186.653910	19.175514	-0.037889	1.074468
197.206010	179.073082	19.180519	-0.037886	1.064468
196.932167	171.561262	19.185523	-0.037830	1.054399
196.860116	164.023545	19.190528	-0.037812	1.044246
196.569018	156.538897	19.195533	-0.037753	1.034013
196.400964	149.034735	19.200538	-0.037718	1.023681
196.503840	141.511538	19.205543	-0.037732	1.013282
196.120660	134.062939	19.210547	-0.037656	1.002761
196.149210	126.566703	19.215552	-0.037657	0.992163
196.018674	119.080558	19.220557	-0.037628	0.981425
196.047843	111.609451	19.225562	-0.037629	0.970630
195.990799	104.177626	19.230567	-0.037614	0.959750
195.666813	96.793045	19.235571	-0.037549	0.948746
195.633936	89.384236	19.240576	-0.037538	0.937652
195.548936	81.994303	19.245581	-0.037518	0.926441
195.553123	74.617254	19.250586	-0.037514	0.915136
195.228245	67.296754	19.255591	-0.037449	0.903688
195.037678	60.202787	19.260595	-0.037409	0.892488