Thu Mar 11 18:43:33 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.507887	-0.005740	0.000000	-0.000014	0.725885

0.557706	-0.024139	0.005005	-0.000024	0.725867
0.181455	0.045814	0.010010	0.000046	0.725873
0.276238	0.026243	0.015014	0.000028	0.725869
0.386577	0.004742	0.020019	0.000007	0.725866
0.349953	0.015035	0.025024	0.000014	0.725874
0.210894	0.033616	0.030029	0.000039	0.725862
0.319060	0.017975	0.035034	0.000019	0.725870
0.360058	0.008697	0.040038	0.000011	0.725867
0.197293	0.036811	0.045043	0.000041	0.725866
0.351725	0.011856	0.050048	0.000012	0.725871
0.381471	0.001625	0.055053	0.000006	0.725862
0.360519	0.009408	0.060058	0.000009	0.725871
0.385591	0.003366	0.065062	0.000004	0.725868
0.337427	0.009601	0.070067	0.000013	0.725864
0.366091	0.008192	0.075072	0.000007	0.725872
0.169294	-0.043323	0.080077	0.000044	0.725703
0.284348	-0.152729	0.085082	0.000022	0.725530
0.430581	-0.178623	0.090086	-0.000005	0.725531
0.359483	-0.168144	0.095091	0.000008	0.725527
0.330981	-0.159897	0.100096	0.000013	0.725534
0.454127	-0.185874	0.105101	-0.000011	0.725527
0.388469	-0.179639	0.110106	0.000001	0.725517
0.180013	-0.296460	0.115110	0.000040	0.725216
0.205212	-0.304401	0.120115	0.000035	0.725210
0.366446	-0.329134	0.125120	0.000004	0.725219
0.126361	-0.290167	0.130125	0.000049	0.725212
0.137800	-0.288912	0.135130	0.000046	0.725219
0.351103	-0.471975	0.140134	0.000006	0.724936
0.322391	-0.492660	0.145139	0.000012	0.724886
0.458247	-0.513955	0.150144	-0.000014	0.724892
0.361813	-0.503034	0.155149	0.000004	0.724880
0.290930	-0.597028	0.160154	0.000017	0.724672
0.234312	-0.628570	0.165158	0.000027	0.724592
0.384320	-0.658089	0.170163	-0.000001	0.724587
0.418890	-0.666339	0.175168	-0.000008	0.724583
0.094585	-0.777803	0.180173	0.000052	0.724252
0.137723	-0.782635	0.185178	0.000044	0.724259
0.357478	-0.821701	0.190182	0.000002	0.724259
0.009535	-0.858745	0.195187	0.000067	0.724066
0.031894	-0.918857	0.200192	0.000062	0.723957
0.215672	-0.957774	0.205197	0.000028	0.723945
0.174290	-1.012226	0.210202	0.000035	0.723825
0.060664	-1.090329	0.215206	0.000056	0.723633
0.133462	-1.104826	0.220211	0.000042	0.723630
0.298944	-1.199067	0.225216	0.000011	0.723504
0.262954	-1.278130	0.230221	0.000018	0.723337
0.493117	-1.316265	0.235226	-0.000025	0.723343
0.438335	-1.446491	0.240230	-0.000015	0.723069
0.248030	-1.448845	0.245235	0.000020	0.722999
0.171391	-1.472308	0.250240	0.000034	0.722926
0.080024	-1.578556	0.255245	0.000050	0.722687
0.169368	-1.590748	0.260250	0.000034	0.722695
0.001441	-1.692590	0.265254	0.000065	0.722437
0.078583	-1.742888	0.270259	0.000050	0.722365
0.207495	-1.824028	0.275264	0.000026	0.722252
0.043038	-1.888216	0.280269	0.000056	0.722069
-0.037080	-1.892493	0.285274	0.000071	0.722033
0.103569	-2.065167	0.290278	0.000044	0.721744
-0.056046	-2.041774	0.295283	0.000074	0.721734
-0.007719	-2.189610	0.300288	0.000064	0.721461
-0.122130	-2.183714	0.305293	0.000085	0.721433
-0.044029	-2.320996	0.310298	0.000071	0.721192
-0.240253	-2.320928	0.315302	0.000107	0.721124
-0.433391	-2.372994	0.320307	0.000142	0.720954
-0.133699	-2.463168	0.325312	0.000086	0.720882
-0.267451	-2.554538	0.330317	0.000111	0.720656
-1.844069	-2.335671	0.335322	0.000404	0.720535
-6.650360	-1.480900	0.340326	0.001298	0.720533
-5.792010	-1.663993	0.345331	0.001138	0.720474
-6.135510	-1.728949	0.350336	0.001202	0.720227
-7.050764	-1.571886	0.355341	0.001372	0.720216
-6.683541	-1.636316	0.360346	0.001303	0.720218
-6.452905	-1.677610	0.365350	0.001260	0.720218
-6.895345	-1.602846	0.370355	0.001342	0.720211
-6.837191	-1.607954	0.375360	0.001331	0.720222
-6.902301	-1.601100	0.380365	0.001343	0.720213
-6.834208	-1.723337	0.385370	0.001330	0.719997
-7.843298	-1.596744	0.390374	0.001517	0.719893
-7.907706	-1.587397	0.395379	0.001529	0.719889
-7.411623	-1.671489	0.400384	0.001436	0.719898
-7.857658	-1.597625	0.405389	0.001519	0.719888
-7.929571	-1.580881	0.410394	0.001532	0.719896
-7.400519	-1.675836	0.415398	0.001433	0.719895
-7.382067	-1.731079	0.420403	0.001430	0.719794
-8.651030	-1.602382	0.425408	0.001665	0.719602
-8.995246	-1.546133	0.430413	0.001729	0.719593
-8.427904	-1.644186	0.435418	0.001623	0.719600
-8.383711	-1.653150	0.440422	0.001615	0.719598
-8.701461	-1.599239	0.445427	0.001674	0.719593
-8.625798	-1.609847	0.450432	0.001659	0.719600
-8.541517	-1.628564	0.455437	0.001643	0.719593
-9.170090	-1.667401	0.460442	0.001760	0.719296
-9.482919	-1.625684	0.465446	0.001818	0.719269
-9.583829	-1.611021	0.470451	0.001836	0.719263
-9.481971	-1.625307	0.475456	0.001817	0.719271
-9.974692	-1.542765	0.480461	0.001908	0.719262
-9.600466	-1.607696	0.485466	0.001838	0.719266
-9.474945	-1.628452	0.490470	0.001815	0.719269
-10.069035	-1.550375	0.495475	0.001925	0.719215
-10.296913	-1.637623	0.500480	0.001967	0.718964
-10.400408	-1.625506	0.505485	0.001986	0.718952
-10.943060	-1.527815	0.510490	0.002087	0.718955
-10.489257	-1.608662	0.515494	0.002002	0.718955
-10.437258	-1.621904	0.520499	0.001992	0.718948
-10.664769	-1.576226	0.525504	0.002034	0.718959
-10.803368	-1.555205	0.530509	0.002060	0.718952
-10.292030	-1.728736	0.535514	0.001964	0.718790
-11.173281	-1.647383	0.540518	0.002128	0.718641
-11.223957	-1.640913	0.545523	0.002137	0.718637
-11.182706	-1.643065	0.550528	0.002129	0.718648
-11.326368	-1.622841	0.555533	0.002155	0.718638
-11.568379	-1.577548	0.560538	0.002200	0.718643
-11.368572	-1.613119	0.565542	0.002163	0.718643
-11.745719	-1.640270	0.570547	0.002233	0.718458
-12.239861	-1.605610	0.575552	0.002324	0.718353
-12.004743	-1.651306	0.580557	0.002280	0.718346
-12.024207	-1.644860	0.585562	0.002284	0.718352
-12.124886	-1.628059	0.590566	0.002302	0.718351
-12.499759	-1.564518	0.595571	0.002371	0.718345
-12.183949	-1.615415	0.600576	0.002312	0.718356
-12.247666	-1.706847	0.605581	0.002324	0.718154
-13.663034	-1.526175	0.610586	0.002587	0.718013
-13.117310	-1.622807	0.615590	0.002485	0.718015
-13.198907	-1.609761	0.620595	0.002500	0.718013
-13.295468	-1.589584	0.625600	0.002518	0.718019
-13.481771	-1.561167	0.630605	0.002552	0.718010
-13.354670	-1.582210	0.635610	0.002528	0.718014
-12.794310	-1.691563	0.640614	0.002423	0.717996
-13.999584	-1.628504	0.645619	0.002648	0.717697
-13.908789	-1.639765	0.650624	0.002630	0.717707
-14.046745	-1.620035	0.655629	0.002656	0.717698
-13.984188	-1.628754	0.660634	0.002644	0.717704
-14.121855	-1.605364	0.665638	0.002669	0.717702
-14.352360	-1.568794	0.670643	0.002712	0.717694
-14.037128	-1.620149	0.675648	0.002653	0.717704
-14.484307	-1.678038	0.680653	0.002736	0.717432
-15.335828	-1.553074	0.685658	0.002894	0.717380
-15.159943	-1.585256	0.690662	0.002861	0.717379
-15.280515	-1.566134	0.695667	0.002883	0.717375
-14.960291	-1.619527	0.700672	0.002823	0.717383
-14.689612	-1.671751	0.705677	0.002772	0.717375
-15.016120	-1.612987	0.710682	0.002833	0.717377
-15.143564	-1.648605	0.715686	0.002856	0.717263
-15.868644	-1.613901	0.720691	0.002991	0.717076
-15.450106	-1.683743	0.725696	0.002913	0.717086
-16.209525	-1.551970	0.730701	0.003054	0.717080
-15.997551	-1.588096	0.735706	0.003014	0.717084
-15.626459	-1.653905	0.740710	0.002944	0.717085
-16.195405	-1.557204	0.745715	0.003050	0.717076
-16.019868	-1.638874	0.750720	0.003017	0.716977
-16.906041	-1.595940	0.755725	0.003182	0.716750
-16.712096	-1.627988	0.760730	0.003145	0.716756
-16.822148	-1.609080	0.765734	0.003166	0.716755
-17.045624	-1.572926	0.770739	0.003207	0.716749
-16.700599	-1.629560	0.775744	0.003142	0.716759
-16.960599	-1.587689	0.780749	0.003190	0.716750
-16.944967	-1.590538	0.785754	0.003187	0.716751
-17.131868	-1.689705	0.790758	0.003222	0.716489
-18.300652	-1.507470	0.795763	0.003439	0.716438
-17.997921	-1.555628	0.800768	0.003382	0.716451
-17.578315	-1.636665	0.805773	0.003304	0.716439
-18.035695	-1.553049	0.810778	0.003389	0.716443
-18.006443	-1.558049	0.815782	0.003383	0.716444
-18.034285	-1.556820	0.820787	0.003388	0.716438
-17.707763	-1.641141	0.825792	0.003327	0.716387
-18.813271	-1.576247	0.830797	0.003532	0.716126
-18.727008	-1.590181	0.835802	0.003516	0.716129
-18.655908	-1.602281	0.840806	0.003502	0.716131
-18.680535	-1.602766	0.845811	0.003507	0.716122
-18.701785	-1.594002	0.850816	0.003510	0.716132
-18.902976	-1.563389	0.855821	0.003547	0.716122
-18.776326	-1.582194	0.860826	0.003523	0.716130
-18.885798	-1.653165	0.865830	0.003543	0.715952
-19.864136	-1.515855	0.870835	0.003725	0.715879
-19.436767	-1.589097	0.875840	0.003645	0.715885
-19.619888	-1.560440	0.880845	0.003679	0.715878
-19.624593	-1.561124	0.885850	0.003680	0.715876
-19.291475	-1.618916	0.890854	0.003617	0.715879
-19.677599	-1.552167	0.895859	0.003689	0.715876
-19.764480	-1.663744	0.900864	0.003705	0.715625
-20.340875	-1.603684	0.905869	0.003812	0.715541
-20.293133	-1.613396	0.910874	0.003803	0.715539
-20.362892	-1.598357	0.915878	0.003815	0.715545
-20.813427	-1.519580	0.920883	0.003899	0.715542
-20.307795	-1.607476	0.925888	0.003804	0.715547
-20.351897	-1.603228	0.930893	0.003812	0.715541
-21.132716	-1.604499	0.935898	0.003957	0.715263
-21.153206	-1.617322	0.940902	0.003961	0.715231
-21.608913	-1.537503	0.945907	0.004045	0.715229
-21.433242	-1.565480	0.950912	0.004012	0.715236
-21.377654	-1.580681	0.955917	0.004002	0.715226
-21.525087	-1.552750	0.960922	0.004029	0.715230
-21.312164	-1.590314	0.965926	0.003989	0.715231
-21.577167	-1.630351	0.970931	0.004038	0.715059
-22.518891	-1.538520	0.975936	0.004213	0.714909
-22.284095	-1.583914	0.980941	0.004169	0.714902
-22.413215	-1.558971	0.985946	0.004193	0.714907
-22.193474	-1.596807	0.990950	0.004151	0.714910
-22.466475	-1.551934	0.995955	0.004202	0.714903
-22.478741	-1.547337	1.000960	0.004204	0.714908
-22.104272	-1.639677	1.005965	0.004134	0.714858
-22.979515	-1.610339	1.010970	0.004297	0.714608
-23.085855	-1.590045	1.015974	0.004316	0.714611
-23.576661	-1.505658	1.020979	0.004407	0.714605
-22.790692	-1.641699	1.025984	0.004261	0.714614
-23.037450	-1.601420	1.030989	0.004306	0.714607
-23.529726	-1.514177	1.035994	0.004397	0.714607
-22.798453	-1.673415	1.040998	0.004261	0.714550
-23.838299	-1.627777	1.046003	0.004454	0.714273
-24.238453	-1.551326	1.051008	0.004528	0.714284
-24.160151	-1.572060	1.056013	0.004514	0.714271
-23.965671	-1.604417	1.061018	0.004477	0.714276
-23.869941	-1.621263	1.066022	0.004459	0.714277
-24.357490	-1.538121	1.071027	0.004549	0.714271
-24.230029	-1.556337	1.076032	0.004525	0.714280
-24.890930	-1.593901	1.081037	0.004648	0.713972
-25.257040	-1.534238	1.086042	0.004716	0.713962
-25.166558	-1.548696	1.091046	0.004699	0.713966
-25.072957	-1.569012	1.096051	0.004681	0.713959
-25.270920	-1.529684	1.101056	0.004718	0.713968
-25.070696	-1.568840	1.106061	0.004680	0.713961
-25.037244	-1.574080	1.111066	0.004673	0.713963
-25.176938	-1.586368	1.116070	0.004699	0.713890
-26.334150	-1.505857	1.121075	0.004914	0.713641
-25.406530	-1.666130	1.126080	0.004741	0.713651
-26.047601	-1.556179	1.131085	0.004860	0.713643
-26.498265	-1.474381	1.136090	0.004944	0.713647
-25.928747	-1.572933	1.141094	0.004838	0.713653
-25.850552	-1.591837	1.146099	0.004823	0.713644
-25.963621	-1.568146	1.151104	0.004843	0.713652
-26.438671	-1.620429	1.156109	0.004932	0.713380
-26.672235	-1.593125	1.161114	0.004975	0.713352
-26.829251	-1.562900	1.166118	0.005004	0.713357
-27.054492	-1.526759	1.171123	0.005045	0.713350
-26.682079	-1.588273	1.176128	0.004976	0.713360
-26.888331	-1.555475	1.181133	0.005014	0.713353
-27.057929	-1.524225	1.186138	0.005045	0.713356
-27.075839	-1.648483	1.191142	0.005048	0.713103
-28.012642	-1.526543	1.196147	0.005222	0.713014
-27.909894	-1.539700	1.201152	0.005203	0.713025
-27.932701	-1.539899	1.206157	0.005207	0.713017
-27.822075	-1.558107	1.211162	0.005186	0.713020
-27.656173	-1.585341	1.216166	0.005154	0.713026
-27.996607	-1.529770	1.221171	0.005217	0.713016
-27.596574	-1.659622	1.226176	0.005143	0.712900
-28.439364	-1.608126	1.231181	0.005299	0.712704
-28.587104	-1.582103	1.236186	0.005327	0.712704
-28.861405	-1.531021	1.241190	0.005377	0.712709
-28.809979	-1.545151	1.246195	0.005367	0.712700
-28.645362	-1.570785	1.251200	0.005336	0.712708
-29.115483	-1.489633	1.256205	0.005424	0.712703
-28.899631	-1.544545	1.261210	0.005383	0.712671
-29.213060	-1.630831	1.266214	0.005441	0.712389
-29.876588	-1.517213	1.271219	0.005564	0.712380
-29.970230	-1.495618	1.276224	0.005581	0.712390
-29.657096	-1.556416	1.281229	0.005523	0.712381
-29.629063	-1.561164	1.286234	0.005517	0.712382
-29.681250	-1.550482	1.291238	0.005527	0.712386
-29.535784	-1.581875	1.296243	0.005499	0.712375
-29.782260	-1.643445	1.301248	0.005545	0.712166
-31.195336	-1.432572	1.306253	0.005808	0.712085
-30.613283	-1.535530	1.311258	0.005699	0.712087
-30.173001	-1.611738	1.316262	0.005617	0.712092
-31.074861	-1.456432	1.321267	0.005784	0.712082
-30.563404	-1.543129	1.326272	0.005689	0.712091
-30.333438	-1.586679	1.331277	0.005646	0.712087
-30.803403	-1.548275	1.336282	0.005733	0.711997
-31.909566	-1.469163	1.341286	0.005938	0.711762
-31.241989	-1.594214	1.346291	0.005814	0.711751
-31.381462	-1.565161	1.351296	0.005840	0.711760
-31.785552	-1.495298	1.356301	0.005914	0.711756
-31.655714	-1.518970	1.361306	0.005890	0.711756
-31.194975	-1.597730	1.366310	0.005804	0.711763
-31.815370	-1.493003	1.371315	0.005919	0.711752
-31.896223	-1.583008	1.376320	0.005934	0.711544
-32.495530	-1.524452	1.381325	0.006045	0.711449
-32.404561	-1.541550	1.386330	0.006028	0.711447
-32.307549	-1.555069	1.391334	0.006009	0.711456
-32.786539	-1.473343	1.396339	0.006098	0.711449
-32.334068	-1.551416	1.401344	0.006014	0.711455
-32.576388	-1.512176	1.406349	0.006059	0.711447
-32.571971	-1.562328	1.411354	0.006057	0.711349
-33.116020	-1.569927	1.416358	0.006158	0.711141
-33.117640	-1.575493	1.421363	0.006158	0.711130
-33.482282	-1.507609	1.426368	0.006226	0.711137
-32.934212	-1.606710	1.431373	0.006124	0.711135
-32.964945	-1.600166	1.436378	0.006129	0.711137
-33.584261	-1.489011	1.441382	0.006244	0.711139
-33.537437	-1.556395	1.446387	0.006235	0.711022
-33.818174	-1.583616	1.451392	0.006287	0.710869
-34.147048	-1.527071	1.456397	0.006348	0.710865
-34.574411	-1.450277	1.461402	0.006427	0.710867
-33.953894	-1.559319	1.466406	0.006311	0.710871
-33.858846	-1.580467	1.471411	0.006293	0.710863
-34.467982	-1.470226	1.476416	0.006406	0.710867
-34.244371	-1.576790	1.481421	0.006364	0.710734
-34.934419	-1.559523	1.486426	0.006493	0.710524
-34.612857	-1.613651	1.491430	0.006432	0.710531
-35.187594	-1.514735	1.496435	0.006539	0.710524
-35.005917	-1.541786	1.501440	0.006505	0.710535
-35.090467	-1.531631	1.506445	0.006520	0.710526
-35.361467	-1.482466	1.511450	0.006571	0.710529
-34.855535	-1.635403	1.516454	0.006476	0.710404
-36.098081	-1.511069	1.521459	0.006707	0.710210
-36.093727	-1.508397	1.526464	0.006706	0.710218
-35.772415	-1.568615	1.531469	0.006646	0.710213
-35.705549	-1.579935	1.536474	0.006633	0.710214
-35.797903	-1.563153	1.541478	0.006650	0.710216
-36.322767	-1.474722	1.546483	0.006747	0.710206
-35.602768	-1.659806	1.551488	0.006613	0.710093
-36.774171	-1.554348	1.556493	0.006831	0.709887
-37.072557	-1.500809	1.561498	0.006886	0.709889
-36.720431	-1.560429	1.566502	0.006820	0.709895
-36.730439	-1.562812	1.571507	0.006822	0.709888
-36.959306	-1.518929	1.576512	0.006864	0.709895
-37.038382	-1.507442	1.581517	0.006878	0.709890
-36.830463	-1.565760	1.586522	0.006839	0.709848
-37.354818	-1.598559	1.591526	0.006937	0.709596
-37.825762	-1.519925	1.596531	0.007024	0.709586
-37.810817	-1.518168	1.601536	0.007021	0.709596
-37.503565	-1.575295	1.606541	0.006963	0.709591
-37.996269	-1.488374	1.611546	0.007055	0.709590
-37.604549	-1.556028	1.616550	0.006982	0.709595
-37.647015	-1.563707	1.621555	0.006989	0.709565
-38.654720	-1.534490	1.626560	0.007177	0.709265
-38.726546	-1.525656	1.631565	0.007190	0.709258
-38.690840	-1.532165	1.636570	0.007183	0.709258
-38.618792	-1.541836	1.641574	0.007169	0.709265
-38.977030	-1.482933	1.646579	0.007235	0.709256
-38.598623	-1.545800	1.651584	0.007165	0.709265
-38.441781	-1.577798	1.656589	0.007135	0.709258
-39.108236	-1.570342	1.661594	0.007259	0.709036
-39.670620	-1.510881	1.666598	0.007363	0.708955
-39.449510	-1.555151	1.671603	0.007322	0.708946
-39.483262	-1.545734	1.676608	0.007328	0.708953
-39.973215	-1.460935	1.681613	0.007419	0.708949
-39.658859	-1.517107	1.686618	0.007360	0.708949
-39.276805	-1.582382	1.691622	0.007288	0.708955
-39.986723	-1.499193	1.696627	0.007420	0.708869
-40.457899	-1.530993	1.701632	0.007508	0.708638
-40.144342	-1.588154	1.706637	0.007449	0.708636
-40.873277	-1.459083	1.711642	0.007584	0.708635
-40.696364	-1.489319	1.716646	0.007551	0.708638
-40.561585	-1.517382	1.721651	0.007526	0.708630
-40.840971	-1.461654	1.726656	0.007577	0.708643
-40.671806	-1.495886	1.731661	0.007545	0.708635
-40.544273	-1.626174	1.736666	0.007521	0.708420
-41.220064	-1.542058	1.741670	0.007647	0.708348
-41.709135	-1.460137	1.746675	0.007738	0.708338
-41.479665	-1.497949	1.751680	0.007695	0.708345
-40.967521	-1.590817	1.756685	0.007599	0.708343
-41.584127	-1.482427	1.761690	0.007713	0.708340
-41.409038	-1.511715	1.766694	0.007681	0.708345
-41.557321	-1.620597	1.771699	0.007708	0.708074
-42.267968	-1.526315	1.776704	0.007840	0.708010
-42.454848	-1.495838	1.781709	0.007874	0.708005
-42.495659	-1.488982	1.786714	0.007882	0.708004
-42.306556	-1.520264	1.791718	0.007846	0.708010
-42.582432	-1.473768	1.796723	0.007897	0.708005
-42.430081	-1.498188	1.801728	0.007868	0.708011
-42.311828	-1.577490	1.806733	0.007846	0.707895
-43.702958	-1.430671	1.811738	0.008105	0.707693
-43.079361	-1.540022	1.816742	0.007988	0.707697
-43.330136	-1.500100	1.821747	0.008035	0.707688
-43.452295	-1.475592	1.826752	0.008057	0.707694
-43.297412	-1.505602	1.831757	0.008028	0.707690
-43.005725	-1.556999	1.836762	0.007973	0.707692
-42.746732	-1.635214	1.841766	0.007925	0.707628
-44.368591	-1.475112	1.846771	0.008227	0.707370
-44.157483	-1.509815	1.851776	0.008187	0.707376
-43.801941	-1.574579	1.856781	0.008120	0.707374
-44.191852	-1.508181	1.861786	0.008193	0.707368
-44.125100	-1.516064	1.866790	0.008180	0.707377
-44.182757	-1.510561	1.871795	0.008190	0.707368
-43.845875	-1.590901	1.876800	0.008127	0.707328
-44.851437	-1.537052	1.881805	0.008314	0.707077
-45.186158	-1.477340	1.886810	0.008376	0.707078
-44.943433	-1.519235	1.891814	0.008331	0.707081
-44.773552	-1.554833	1.896819	0.008299	0.707071
-44.599488	-1.580213	1.901824	0.008266	0.707083
-44.916891	-1.526542	1.906829	0.008325	0.707078
-45.025909	-1.544886	1.911834	0.008345	0.707002
-45.842320	-1.523095	1.916838	0.008497	0.706755
-45.770584	-1.541080	1.921843	0.008483	0.706745
-45.932827	-1.508031	1.926848	0.008513	0.706754
-46.050820	-1.489165	1.931853	0.008534	0.706750
-45.934704	-1.509854	1.936858	0.008512	0.706750
-45.589144	-1.568839	1.941862	0.008448	0.706756
-45.934406	-1.518515	1.946867	0.008512	0.706734
-46.849924	-1.498309	1.951872	0.008682	0.706448
-46.581742	-1.548475	1.956877	0.008632	0.706444
-46.861518	-1.499953	1.961882	0.008683	0.706441
-46.713732	-1.522559	1.966886	0.008656	0.706450
-46.735960	-1.524414	1.971891	0.008659	0.706438
-46.542279	-1.555007	1.976896	0.008623	0.706447
-46.428030	-1.584918	1.981901	0.008602	0.706428
-47.619345	-1.524139	1.986906	0.008823	0.706124
-47.366137	-1.567287	1.991910	0.008776	0.706129
-47.745770	-1.501584	1.996915	0.008846	0.706126
-47.535866	-1.537287	2.001920	0.008807	0.706130

-47.583013	-1.528941	2.011917	0.008815	0.706131
-47.562702	-1.554154	2.021914	0.008810	0.706089
-48.504266	-1.499417	2.031910	0.008985	0.705862
-48.371952	-1.524500	2.041907	0.008960	0.705860
-48.356631	-1.525346	2.051904	0.008956	0.705865
-48.213259	-1.552634	2.061901	0.008929	0.705863
-47.881372	-1.485977	2.071898	0.008866	0.706117
-47.757928	-1.503532	2.081894	0.008843	0.706128
-47.521182	-1.546220	2.091891	0.008798	0.706128
-47.668840	-1.520112	2.101888	0.008825	0.706129
-47.633185	-1.527770	2.111885	0.008818	0.706127
-47.413577	-1.568025	2.121882	0.008776	0.706126
-47.731331	-1.511363	2.131878	0.008835	0.706127
-47.549041	-1.546054	2.141875	0.008800	0.706124
-47.504510	-1.475172	2.151872	0.008791	0.706284
-46.559521	-1.563385	2.161869	0.008615	0.706446
-47.069629	-1.473990	2.171866	0.008709	0.706444
-46.756685	-1.531194	2.181862	0.008650	0.706443
-46.823249	-1.509080	2.191859	0.008662	0.706465
-45.994018	-1.514778	2.201856	0.008507	0.706751
-45.894972	-1.532608	2.211853	0.008488	0.706752
-45.885613	-1.535073	2.221850	0.008485	0.706752
-45.887343	-1.535250	2.231846	0.008485	0.706752
-45.223106	-1.493646	2.241843	0.008361	0.707075
-45.008875	-1.526323	2.251840	0.008320	0.707087
-44.882999	-1.549285	2.261837	0.008296	0.707087
-45.315434	-1.448710	2.271834	0.008376	0.707135
-44.221685	-1.525671	2.281830	0.008172	0.707373
-44.344495	-1.503059	2.291827	0.008194	0.707376
-44.357794	-1.499889	2.301824	0.008196	0.707379
-43.493276	-1.541944	2.311821	0.008034	0.707605
-43.498031	-1.494558	2.321818	0.008035	0.707700
-43.509405	-1.492549	2.331814	0.008036	0.707701
-43.474305	-1.472991	2.341811	0.008029	0.707754
-42.509479	-1.516136	2.351808	0.007849	0.708013
-42.330340	-1.548863	2.361805	0.007815	0.708013
-42.705311	-1.481306	2.371802	0.007884	0.708015
-42.063795	-1.495550	2.381798	0.007764	0.708217
-41.525747	-1.527708	2.391795	0.007663	0.708346
-41.485735	-1.533609	2.401792	0.007655	0.708350
-41.525084	-1.528017	2.411789	0.007662	0.708348
-40.922416	-1.503489	2.421786	0.007549	0.708614
-40.775908	-1.518031	2.431782	0.007521	0.708638
-40.553543	-1.557992	2.441779	0.007479	0.708639
-40.678697	-1.478540	2.451776	0.007501	0.708754
-39.734541	-1.546137	2.461773	0.007325	0.708957
-40.198127	-1.465210	2.471770	0.007411	0.708955
-39.891707	-1.515896	2.481766	0.007353	0.708964
-39.184703	-1.492968	2.491763	0.007221	0.709263
-39.049099	-1.517347	2.501760	0.007195	0.709264
-38.917940	-1.540270	2.511757	0.007170	0.709266
-38.806173	-1.460062	2.521754	0.007148	0.709468
-38.112114	-1.519702	2.531750	0.007018	0.709597
-38.317491	-1.482335	2.541747	0.007056	0.709600
-38.236598	-1.468049	2.551744	0.007040	0.709659
-37.429654	-1.492559	2.561741	0.006890	0.709898
-37.246090	-1.526813	2.571738	0.006855	0.709896
-37.320779	-1.513284	2.581734	0.006868	0.709898
-36.995617	-1.444070	2.591731	0.006807	0.710153
-36.546005	-1.491754	2.601728	0.006722	0.710220
-36.386276	-1.521134	2.611725	0.006692	0.710219
-36.519196	-1.428079	2.621722	0.006716	0.710359
-35.550761	-1.515826	2.631718	0.006535	0.710529
-35.711182	-1.486510	2.641715	0.006564	0.710532
-35.449356	-1.533497	2.651712	0.006515	0.710533
-34.737664	-1.493312	2.661709	0.006382	0.710867
-34.647983	-1.509152	2.671706	0.006365	0.710869
-34.529386	-1.531084	2.681702	0.006342	0.710868
-34.811028	-1.437887	2.691699	0.006394	0.710955
-33.750083	-1.535810	2.701696	0.006196	0.711139
-33.929670	-1.503510	2.711693	0.006228	0.711140
-33.952483	-1.501026	2.721690	0.006232	0.711138
-33.194174	-1.482039	2.731686	0.006090	0.711447
-33.140806	-1.488116	2.741683	0.006080	0.711455
-32.904557	-1.531129	2.751680	0.006035	0.711455
-32.929779	-1.432452	2.761677	0.006039	0.711644
-32.015668	-1.538681	2.771674	0.005868	0.711758
-32.293726	-1.490520	2.781670	0.005919	0.711756
-32.171147	-1.477216	2.791667	0.005896	0.711827
-31.184758	-1.523021	2.801664	0.005712	0.712088
-31.304444	-1.502179	2.811661	0.005733	0.712088
-31.353067	-1.493725	2.821658	0.005742	0.712089
-30.612490	-1.516272	2.831654	0.005603	0.712308
-30.470391	-1.504297	2.841651	0.005576	0.712383
-30.256936	-1.541953	2.851648	0.005536	0.712385
-30.591377	-1.447417	2.861645	0.005597	0.712456
-29.464242	-1.522568	2.871642	0.005387	0.712708
-29.735120	-1.475691	2.881638	0.005437	0.712706
-29.643920	-1.492072	2.891635	0.005419	0.712707
-28.791448	-1.509948	2.901632	0.005260	0.712975
-28.625161	-1.517403	2.911629	0.005228	0.713020
-28.650232	-1.513263	2.921626	0.005232	0.713021
-28.713049	-1.462106	2.931622	0.005243	0.713102
-27.909406	-1.477959	2.941619	0.005093	0.713356
-27.603877	-1.531426	2.951616	0.005035	0.713359
-27.963853	-1.469384	2.961613	0.005102	0.713356
-27.074220	-1.503768	2.971610	0.004936	0.713604
-27.209132	-1.459778	2.981606	0.004960	0.713645
-26.747078	-1.541248	2.991603	0.004873	0.713648
-26.966249	-1.439397	3.001600	0.004914	0.713774
-26.146225	-1.487253	3.011597	0.004760	0.713971
-26.042608	-1.507221	3.021594	0.004740	0.713969
-26.012166	-1.515566	3.031590	0.004734	0.713964
-25.398881	-1.479394	3.041587	0.004619	0.714254
-25.248696	-1.496092	3.051584	0.004591	0.714276
-25.232959	-1.498396	3.061581	0.004587	0.714278
-24.797975	-1.494379	3.071578	0.004505	0.714441
-24.448891	-1.475314	3.081574	0.004440	0.714603
-24.099523	-1.537134	3.091571	0.004374	0.714605
-24.520923	-1.461520	3.101568	0.004452	0.714608
-23.439160	-1.509887	3.111565	0.004250	0.714895
-23.512373	-1.492484	3.121562	0.004263	0.714905
-23.515002	-1.494429	3.131558	0.004263	0.714902
-23.248486	-1.471074	3.141555	0.004212	0.715043
-22.625588	-1.487673	3.151552	0.004096	0.715232
-22.513132	-1.508308	3.161549	0.004074	0.715232
-22.634586	-1.488574	3.171546	0.004096	0.715229
-21.909637	-1.461135	3.181542	0.003961	0.715541
-21.572491	-1.521797	3.191539	0.003897	0.715541
-21.779314	-1.483585	3.201536	0.003935	0.715545
-21.085476	-1.530133	3.211533	0.003805	0.715699
-20.653793	-1.516437	3.221530	0.003724	0.715880
-20.670956	-1.514533	3.231526	0.003727	0.715879
-20.810229	-1.489418	3.241523	0.003752	0.715880
-20.223538	-1.500352	3.251520	0.003642	0.716067
-19.921625	-1.522626	3.261517	0.003585	0.716131
-20.232616	-1.468145	3.271514	0.003643	0.716130
-19.784139	-1.490682	3.281510	0.003559	0.716245
-18.843500	-1.556521	3.291507	0.003383	0.716447
-18.943491	-1.540061	3.301504	0.003401	0.716446
-18.849091	-1.557834	3.311501	0.003383	0.716445
-18.489533	-1.504814	3.321498	0.003315	0.716678
-18.071812	-1.540894	3.331494	0.003237	0.716755
-18.228256	-1.513866	3.341491	0.003265	0.716755
-18.154104	-1.474369	3.351488	0.003251	0.716860
-17.048148	-1.556993	3.361485	0.003044	0.717088
-17.273094	-1.517369	3.371482	0.003085	0.717088
-16.990266	-1.571549	3.381478	0.003032	0.717082
-16.772407	-1.515859	3.391475	0.002991	0.717270
-16.437573	-1.522279	3.401472	0.002928	0.717376
-16.358041	-1.534478	3.411469	0.002913	0.717381
-16.291924	-1.527057	3.421466	0.002900	0.717421
-15.498601	-1.527838	3.431462	0.002751	0.717700
-15.421500	-1.540117	3.441459	0.002736	0.717704
-15.351279	-1.552396	3.451456	0.002723	0.717705
-14.789557	-1.565813	3.461453	0.002617	0.717878
-14.389790	-1.566778	3.471450	0.002542	0.718018
-14.374509	-1.571684	3.481446	0.002539	0.718015
-14.576990	-1.537211	3.491443	0.002576	0.718013
-13.747264	-1.555467	3.501440	0.002421	0.718270
-13.352611	-1.583619	3.511437	0.002347	0.718354
-13.549435	-1.550353	3.521434	0.002383	0.718352
-13.637276	-1.522803	3.531430	0.002398	0.718376
-12.703061	-1.555954	3.541427	0.002224	0.718641
-12.378215	-1.611878	3.551424	0.002163	0.718646
-12.541790	-1.583545	3.561421	0.002193	0.718645
-12.569715	-1.515025	3.571418	0.002197	0.718772
-11.460043	-1.618007	3.581414	0.001990	0.718960
-11.978791	-1.525942	3.591411	0.002086	0.718960
-11.713270	-1.573002	3.601408	0.002036	0.718962
-11.173075	-1.536927	3.611405	0.001935	0.719224
-10.794620	-1.580558	3.621402	0.001863	0.719272
-10.740640	-1.593191	3.631398	0.001853	0.719267
-10.729790	-1.562871	3.641395	0.001850	0.719332
-9.795107	-1.594836	3.651392	0.001675	0.719598
-9.486257	-1.650917	3.661389	0.001617	0.719598
-9.892193	-1.579304	3.671386	0.001692	0.719597
-9.582976	-1.574029	3.681382	0.001634	0.719717
-9.001378	-1.588454	3.691379	0.001525	0.719894
-8.981823	-1.591269	3.701376	0.001521	0.719897
-9.278603	-1.539573	3.711373	0.001575	0.719896
-8.353802	-1.545613	3.721370	0.001403	0.720209
-8.012157	-1.603009	3.731366	0.001338	0.720217
-8.111548	-1.584879	3.741363	0.001356	0.720219
-8.098208	-1.521695	3.751360	0.001353	0.720350
-6.967104	-1.627458	3.761357	0.001142	0.720539
-7.242608	-1.581022	3.771354	0.001193	0.720535
-7.169206	-1.594775	3.781350	0.001178	0.720535
-6.580276	-1.563527	3.791347	0.001068	0.720804
-6.022118	-1.627259	3.801344	0.000963	0.720876
-6.228126	-1.590381	3.811341	0.001001	0.720877
-6.128068	-1.608721	3.821338	0.000982	0.720877
-5.783985	-1.549061	3.831334	0.000917	0.721116
-5.367479	-1.622282	3.841331	0.000839	0.721119
-5.406260	-1.615739	3.851328	0.000846	0.721120
-5.008865	-1.593154	3.861325	0.000771	0.721305
-4.466059	-1.623074	3.871322	0.000669	0.721437
-4.599409	-1.598777	3.881318	0.000694	0.721439
-4.702037	-1.569773	3.891315	0.000712	0.721461
-3.698781	-1.604436	3.901312	0.000525	0.721746
-3.943735	-1.561141	3.911309	0.000570	0.721746
-3.920780	-1.566626	3.921306	0.000565	0.721745
-3.201177	-1.568503	3.931302	0.000430	0.721994
-2.931946	-1.576737	3.941299	0.000379	0.722073
-2.877377	-1.586100	3.951296	0.000368	0.722075
-2.814087	-1.544765	3.961293	0.000356	0.722179
-2.581558	-1.489968	3.971290	0.000312	0.722369
-2.201845	-1.558777	3.981286	0.000241	0.722368
-2.327878	-1.492747	3.991283	0.000264	0.722455
-1.607960	-1.499682	4.001280	0.000129	0.722694
-1.424587	-1.532615	4.011277	0.000094	0.722695
-1.499882	-1.493204	4.021274	0.000108	0.722747
-1.379945	-1.384094	4.031270	0.000084	0.723004
-1.381690	-1.384465	4.041267	0.000084	0.723004
-1.284329	-1.303373	4.051264	0.000065	0.723198
-1.001444	-1.281238	4.061261	0.000012	0.723341
-1.044047	-1.235544	4.071258	0.000019	0.723417
-0.831580	-1.164519	4.081254	-0.000021	0.723632
-1.088696	-1.090190	4.091251	0.000026	0.723689
-1.126395	-0.948772	4.101248	0.000033	0.723954
-1.271502	-0.851836	4.111245	0.000059	0.724095
-0.919688	-0.829745	4.121242	-0.000007	0.724262
-0.865160	-0.703560	4.131238	-0.000018	0.724529
-0.637014	-0.680805	4.141235	-0.000061	0.724654
-0.543752	-0.576423	4.151232	-0.000079	0.724892
-0.566162	-0.460199	4.161229	-0.000076	0.725113
-0.746180	-0.328835	4.171226	-0.000043	0.725308
-0.702908	-0.224239	4.181222	-0.000052	0.725529
-0.805270	-0.038164	4.191219	-0.000033	0.725858
-0.414910	-0.005513	4.201216	-0.000107	0.726059
-0.369483	0.102580	4.211213	-0.000116	0.726287
0.000000	0.192539	4.221210	-0.000185	0.726592

-0.135540	0.857081	4.226214	-0.000161	0.727841
-0.144062	2.131092	4.231219	-0.000161	0.730317
0.145411	3.953056	4.236224	-0.000216	0.733946
0.258939	6.348319	4.241229	-0.000239	0.738598
0.459961	9.243101	4.246234	-0.000279	0.744204
1.122175	12.557902	4.251238	-0.000404	0.750716
1.495838	16.358941	4.256243	-0.000477	0.757986
1.885822	20.573927	4.261248	-0.000552	0.765959
2.586397	25.144196	4.266253	-0.000686	0.774602
3.282285	30.075049	4.271258	-0.000819	0.783799
4.062840	35.359563	4.276262	-0.000968	0.793549
4.509427	40.994209	4.281267	-0.001055	0.803694
5.064286	46.932969	4.286272	-0.001163	0.814275
5.480604	53.156191	4.291277	-0.001245	0.825166
5.897507	59.669951	4.296282	-0.001327	0.836409
6.551722	66.343473	4.301286	-0.001454	0.847839
7.526000	73.188517	4.306291	-0.001640	0.859493
8.041188	80.333307	4.311296	-0.001741	0.871347
8.908852	87.592972	4.316301	-0.001907	0.883325
9.866463	95.023346	4.321306	-0.002091	0.895438
10.728209	102.638763	4.326310	-0.002256	0.907651
11.569394	110.395097	4.331315	-0.002418	0.919913
12.394467	118.277695	4.336320	-0.002577	0.932201
13.075146	126.296406	4.341325	-0.002710	0.944495
13.622957	134.449820	4.346330	-0.002817	0.956796
14.574372	142.614912	4.351334	-0.003000	0.969061
15.598095	150.851705	4.356339	-0.003196	0.981293
16.428835	159.233620	4.361344	-0.003357	0.993534
17.534831	167.584455	4.366349	-0.003569	1.005648
18.286675	176.048529	4.371354	-0.003714	1.017690
18.888224	184.586874	4.376358	-0.003832	1.029657
19.674563	193.108465	4.381363	-0.003985	1.041506
20.659442	201.647953	4.386368	-0.004174	1.053293
21.412074	210.241454	4.391373	-0.004320	1.064966
22.265023	218.860049	4.396378	-0.004485	1.076569
23.447300	227.410792	4.401382	-0.004711	1.088033
24.262427	236.044929	4.406387	-0.004868	1.099402
24.912099	244.720006	4.411392	-0.004995	1.110671
25.488003	253.391189	4.416397	-0.005109	1.121806
26.275202	262.027439	4.421402	-0.005261	1.132832
26.885349	270.699156	4.426406	-0.005381	1.143758
27.293312	279.420862	4.431411	-0.005463	1.154599
27.981214	288.041502	4.436416	-0.005597	1.165274
28.841509	296.631953	4.441421	-0.005763	1.175851
29.313388	305.270077	4.446426	-0.005857	1.186311
30.596086	313.790183	4.451430	-0.006101	1.196703
31.172582	322.375479	4.456435	-0.006215	1.206941
31.754627	330.989406	4.461440	-0.006329	1.217126
32.226638	339.582313	4.466445	-0.006423	1.227181
33.087147	348.118107	4.471450	-0.006589	1.237164
33.785777	356.643401	4.476454	-0.006725	1.247024
34.419337	365.176261	4.481459	-0.006849	1.256802
35.329143	373.656344	4.486464	-0.007024	1.266497
35.877248	382.193654	4.491469	-0.007132	1.276114
36.195276	390.723543	4.496474	-0.007197	1.285608
37.225439	399.150018	4.501478	-0.007394	1.295051
37.677459	407.649691	4.506483	-0.007484	1.304398
38.325864	416.213246	4.511488	-0.007611	1.313783
39.090754	424.632609	4.516493	-0.007759	1.322968
39.590446	433.067364	4.521498	-0.007858	1.332058
40.185380	441.475876	4.526502	-0.007975	1.341075
40.345566	449.943909	4.531507	-0.008010	1.350019
40.736755	458.362639	4.536512	-0.008089	1.358892
41.205278	466.743301	4.541517	-0.008182	1.367681
41.641591	475.137342	4.546522	-0.008269	1.376422
42.343103	483.474739	4.551526	-0.008405	1.385095
42.904091	491.852920	4.556531	-0.008516	1.393731
43.462117	500.190529	4.561536	-0.008625	1.402273
44.032228	508.514604	4.566541	-0.008737	1.410751
44.521809	516.853717	4.571546	-0.008834	1.419180
45.079575	525.179546	4.576550	-0.008944	1.427556
45.321951	533.546890	4.581555	-0.008995	1.435874
45.891216	541.838499	4.586560	-0.009106	1.444122
46.451501	550.145284	4.591565	-0.009216	1.452336
46.836533	558.466134	4.596570	-0.009294	1.460489
47.476755	566.759826	4.601574	-0.009419	1.468611
48.197442	575.051858	4.606579	-0.009559	1.476700
48.718328	583.318696	4.611584	-0.009661	1.484688
48.943795	591.647875	4.616589	-0.009709	1.492647
49.756554	599.860126	4.621594	-0.009866	1.500544
50.377736	608.121237	4.626598	-0.009987	1.508416
50.303657	616.471297	4.631603	-0.009979	1.516224
50.775068	624.720179	4.636608	-0.010073	1.523981
51.452510	632.944151	4.641613	-0.010205	1.531706
52.098597	641.163373	4.646618	-0.010331	1.539382
52.424868	649.453487	4.651622	-0.010397	1.547038
52.945568	657.706864	4.656627	-0.010500	1.554652
53.557327	665.917092	4.661632	-0.010619	1.562202
53.959668	674.159615	4.666637	-0.010700	1.569714
54.509490	682.399072	4.671642	-0.010808	1.577209
55.104171	690.608315	4.676646	-0.010924	1.584648
55.412902	698.864997	4.681651	-0.010988	1.592053
56.027095	707.066655	4.686656	-0.011108	1.599419
56.735978	715.235531	4.691661	-0.011245	1.606735
56.837745	723.517424	4.696666	-0.011270	1.614031
57.398351	731.714874	4.701670	-0.011380	1.621285
57.841342	739.926341	4.706675	-0.011468	1.628502
58.418425	748.161663	4.711680	-0.011581	1.635726
59.042578	756.316993	4.716685	-0.011703	1.642856
59.353750	764.527433	4.721690	-0.011767	1.649959
60.050867	772.699075	4.726694	-0.011902	1.657051
60.051440	780.940729	4.731699	-0.011908	1.664078
60.119175	789.194636	4.736704	-0.011926	1.671095
60.763901	797.336746	4.741709	-0.012052	1.678066
61.374040	805.468941	4.746714	-0.012171	1.684994
62.179538	813.620635	4.751718	-0.012327	1.691936
62.571343	821.810037	4.756723	-0.012405	1.698826
63.035261	829.980201	4.761728	-0.012497	1.705682
63.721056	838.153153	4.766733	-0.012631	1.712541
63.907504	846.350603	4.771738	-0.012671	1.719328
64.262071	854.537322	4.776742	-0.012743	1.726102
64.488471	862.740412	4.781747	-0.012791	1.732845
64.997709	870.885165	4.786752	-0.012891	1.739552
65.333798	879.048185	4.791757	-0.012959	1.746225
65.531300	887.259062	4.796762	-0.013002	1.752893
66.212668	895.381454	4.801766	-0.013134	1.759526
66.602313	903.525391	4.806771	-0.013212	1.766114
66.940928	911.716906	4.811776	-0.013281	1.772710
67.222308	919.885610	4.816781	-0.013339	1.779256
67.512543	928.039218	4.821786	-0.013399	1.785767
68.195832	936.207770	4.826790	-0.013532	1.792314
68.828732	944.328600	4.831795	-0.013655	1.798793
69.179074	952.462957	4.836800	-0.013726	1.805225
69.598237	960.605666	4.841805	-0.013810	1.811649
70.017757	968.745373	4.846810	-0.013893	1.818048
70.156523	976.922257	4.851814	-0.013925	1.824419
70.510503	985.058006	4.856819	-0.013996	1.830762
71.163709	993.166595	4.861824	-0.014124	1.837098
71.435145	1001.315278	4.866829	-0.014180	1.843397
71.678539	1009.466634	4.871834	-0.014231	1.849674
71.891170	1017.645733	4.876838	-0.014276	1.855947
71.975161	1025.796827	4.881843	-0.014297	1.862162
72.579680	1033.893672	4.886848	-0.014415	1.868376
73.161546	1042.023782	4.891853	-0.014529	1.874592
73.628455	1050.115763	4.896858	-0.014622	1.880745
74.092031	1058.241444	4.901862	-0.014714	1.886903
74.213499	1066.414998	4.906867	-0.014742	1.893037
74.809094	1074.492328	4.911872	-0.014858	1.899133
74.971194	1082.643813	4.916877	-0.014894	1.905217
75.260111	1090.786509	4.921882	-0.014954	1.911288
75.689419	1098.910463	4.926886	-0.015039	1.917342
76.066729	1107.003003	4.931891	-0.015115	1.923348
76.566694	1115.113761	4.936896	-0.015214	1.929362
76.835550	1123.267802	4.941901	-0.015269	1.935363
77.201998	1131.374055	4.946906	-0.015343	1.941321
77.429316	1139.524305	4.951910	-0.015391	1.947278
77.521595	1147.710081	4.956915	-0.015414	1.953228
78.063949	1155.783467	4.961920	-0.015521	1.959127
78.183249	1163.900968	4.966925	-0.015548	1.964995
78.283842	1172.020649	4.971930	-0.015573	1.970844
78.664891	1180.133830	4.976934	-0.015649	1.976702
78.981345	1188.210406	4.981939	-0.015714	1.982509
79.165947	1196.336277	4.986944	-0.015754	1.988320
79.557329	1204.461301	4.991949	-0.015832	1.994135
80.022696	1212.505641	4.996954	-0.015925	1.999884
80.518103	1220.599614	5.001958	-0.016022	2.005655
80.740723	1228.720435	5.006963	-0.016069	2.011399
81.334053	1236.803189	5.011968	-0.016186	2.017139
81.500944	1244.927358	5.016973	-0.016222	2.022847
81.772272	1253.033720	5.021978	-0.016278	2.028537
82.169805	1261.181081	5.026982	-0.016358	2.034253
82.561799	1269.230533	5.031987	-0.016437	2.039884
82.683547	1277.344512	5.036992	-0.016465	2.045517
82.813865	1285.470665	5.041997	-0.016495	2.051143
83.305439	1293.544328	5.047002	-0.016592	2.056755
83.543887	1301.653132	5.052006	-0.016642	2.062349
83.697730	1309.747698	5.057011	-0.016676	2.067911
84.167107	1317.853394	5.062016	-0.016769	2.073496
84.509983	1325.940812	5.067021	-0.016838	2.079041
84.786722	1334.009593	5.072026	-0.016896	2.084552
85.202439	1342.111362	5.077030	-0.016979	2.090085
85.452249	1350.222252	5.082035	-0.017031	2.095592
85.872671	1358.293109	5.087040	-0.017114	2.101075
86.073223	1366.413026	5.092045	-0.017157	2.106555
86.442192	1374.539943	5.097050	-0.017232	2.112042
86.965899	1382.633956	5.102054	-0.017335	2.117507
87.091275	1390.701531	5.107059	-0.017364	2.122903
87.524440	1398.769399	5.112064	-0.017450	2.128314
87.875616	1406.882645	5.117069	-0.017521	2.133733
88.037533	1414.955689	5.122074	-0.017557	2.139095
88.534223	1423.012026	5.127078	-0.017655	2.144463
89.077306	1431.066171	5.132083	-0.017761	2.149821
89.462391	1439.173407	5.137088	-0.017839	2.155185
89.674926	1447.260455	5.142093	-0.017884	2.160507
90.017062	1455.336714	5.147098	-0.017953	2.165820
90.507339	1463.438345	5.152102	-0.018050	2.171151
90.566654	1471.547558	5.157107	-0.018067	2.176434
90.836845	1479.634559	5.162112	-0.018123	2.181708
91.398305	1487.692576	5.167117	-0.018233	2.186978
91.512845	1495.828162	5.172122	-0.018260	2.192245
91.893677	1503.911816	5.177126	-0.018336	2.197489
92.182289	1511.962219	5.182131	-0.018395	2.202691
92.631011	1520.023927	5.187136	-0.018485	2.207903
92.860106	1528.134478	5.192141	-0.018533	2.213114
93.158070	1536.198093	5.197146	-0.018594	2.218288
93.386945	1544.285312	5.202150	-0.018642	2.223459
93.641729	1552.374872	5.207155	-0.018695	2.228622
94.101634	1560.447277	5.212160	-0.018786	2.233781
94.714232	1568.475829	5.217165	-0.018906	2.238913
94.958589	1576.540979	5.222170	-0.018957	2.244024
95.539649	1584.614753	5.227174	-0.019071	2.249158
95.875638	1592.710918	5.232179	-0.019139	2.254273
96.230631	1600.788920	5.237184	-0.019211	2.259366
96.484973	1608.860650	5.242189	-0.019264	2.264436
96.902042	1616.948393	5.247194	-0.019347	2.269518
97.169230	1625.120511	5.252198	-0.019402	2.274628
97.298618	1633.166204	5.257203	-0.019432	2.279636
97.481664	1641.233383	5.262208	-0.019472	2.284651
97.812422	1649.285938	5.267213	-0.019539	2.289659
97.887405	1657.381441	5.272218	-0.019558	2.294661
98.387067	1665.423610	5.277222	-0.019657	2.299654
98.458904	1673.495532	5.282227	-0.019676	2.304619
98.884223	1681.554067	5.287232	-0.019761	2.309595
99.226928	1689.645426	5.292237	-0.019830	2.314573
99.617944	1697.674883	5.297242	-0.019908	2.319506
100.129941	1705.727528	5.302246	-0.020009	2.324453
100.276647	1713.801188	5.307251	-0.020042	2.329372
100.626220	1721.893538	5.312256	-0.020113	2.334309
100.864432	1729.968309	5.317261	-0.020163	2.339216
100.996195	1738.044894	5.322266	-0.020193	2.344104
101.330705	1746.125491	5.327270	-0.020261	2.349001
101.800986	1754.199107	5.332275	-0.020354	2.353895
102.063583	1762.238495	5.337280	-0.020408	2.358741
102.290081	1770.314346	5.342285	-0.020456	2.363596
102.391219	1778.390388	5.347290	-0.020480	2.368431
102.932242	1786.455021	5.352294	-0.020587	2.373285
103.144168	1794.506183	5.357299	-0.020632	2.378094
103.216977	1802.599819	5.362304	-0.020651	2.382908
103.375123	1810.679739	5.367309	-0.020686	2.387710
103.782665	1818.736618	5.372314	-0.020767	2.392509
104.298347	1826.780697	5.377318	-0.020869	2.397299
104.314298	1834.842878	5.382323	-0.020877	2.402051
104.706590	1842.896980	5.387328	-0.020956	2.406819
105.028556	1850.976138	5.392333	-0.021022	2.411586
105.106959	1859.069692	5.397338	-0.021042	2.416333
105.796699	1867.073602	5.402342	-0.021176	2.421065
106.073921	1875.125737	5.407347	-0.021233	2.425785
106.081839	1883.263682	5.412352	-0.021240	2.430524
106.646267	1891.336564	5.417357	-0.021351	2.435260
106.770347	1899.377423	5.422362	-0.021379	2.439933
106.981215	1907.420483	5.427366	-0.021424	2.444606
107.252641	1915.459494	5.432371	-0.021480	2.449272
107.736955	1923.509665	5.437376	-0.021576	2.453951
108.067830	1931.569835	5.442381	-0.021643	2.458616
108.185350	1939.613880	5.447386	-0.021671	2.463246
108.572003	1947.684593	5.452390	-0.021748	2.467903
109.058810	1955.726356	5.457395	-0.021844	2.472542
109.061967	1963.828464	5.462400	-0.021851	2.477171
109.384264	1971.865613	5.467405	-0.021916	2.481778
109.540255	1979.917262	5.472410	-0.021951	2.486372
110.033647	1987.993539	5.477414	-0.022048	2.490997
110.338661	1996.021075	5.482419	-0.022111	2.495571
110.552588	2004.088288	5.487424	-0.022156	2.500153
110.936224	2012.126699	5.492429	-0.022233	2.504722
111.208627	2020.201021	5.497434	-0.022289	2.509295
111.745099	2028.289318	5.502438	-0.022395	2.513887
112.090368	2036.320257	5.507443	-0.022465	2.518424
112.423647	2044.344597	5.512448	-0.022532	2.522948
112.688970	2052.409565	5.517453	-0.022587	2.527482
112.924266	2060.475694	5.522458	-0.022637	2.532007
113.375856	2068.530198	5.527462	-0.022726	2.536532
113.680549	2076.585549	5.532467	-0.022788	2.541039
113.821728	2084.643886	5.537472	-0.022820	2.545528
114.144013	2092.729576	5.542477	-0.022886	2.550037
114.235307	2100.800136	5.547482	-0.022908	2.554514
114.646904	2108.828802	5.552486	-0.022991	2.558982
114.645318	2116.893733	5.557491	-0.022996	2.563433
114.945154	2124.944835	5.562496	-0.023057	2.567890
115.133968	2133.023832	5.567501	-0.023098	2.572346
115.560920	2141.044301	5.572506	-0.023183	2.576780
115.762875	2149.111410	5.577510	-0.023226	2.581215
115.795181	2157.156427	5.582515	-0.023238	2.585619
116.035597	2165.241455	5.587520	-0.023288	2.590052
116.472669	2173.480639	5.592525	-0.023375	2.594575
116.485889	2181.462227	5.597530	-0.023383	2.598920
116.827620	2189.448418	5.602534	-0.023452	2.603284
116.964566	2197.466236	5.607539	-0.023483	2.607643
117.467893	2205.477393	5.612544	-0.023583	2.612016
117.762935	2213.535655	5.617549	-0.023643	2.616392
117.956189	2221.566090	5.622554	-0.023685	2.620740
118.271867	2229.596864	5.627558	-0.023749	2.625089
118.405502	2237.658708	5.632563	-0.023780	2.629435
118.720151	2245.710197	5.637568	-0.023844	2.633780
119.208672	2253.729874	5.642573	-0.023940	2.638113
119.279078	2261.780302	5.647578	-0.023959	2.642427
119.687512	2269.833132	5.652582	-0.024040	2.646758
119.908816	2277.881055	5.657587	-0.024087	2.651067
120.001088	2285.979119	5.662592	-0.024110	2.655387
120.482145	2293.979480	5.667597	-0.024205	2.659673
120.762504	2302.007518	5.672602	-0.024263	2.663954
121.113752	2310.077733	5.677606	-0.024334	2.668255
121.238202	2318.174003	5.682611	-0.024363	2.672548
121.608233	2326.214534	5.687616	-0.024437	2.676820
121.902926	2334.241733	5.692621	-0.024497	2.681074
122.163886	2342.258062	5.697626	-0.024552	2.685313
122.331456	2350.328804	5.702630	-0.024588	2.689568
122.636440	2358.394669	5.707635	-0.024651	2.693822
122.879128	2366.429715	5.712640	-0.024701	2.698050
123.036196	2374.484226	5.717645	-0.024736	2.702275
123.172352	2382.510905	5.722650	-0.024767	2.706478
123.358445	2390.596264	5.727654	-0.024807	2.710709
123.542733	2398.650804	5.732659	-0.024847	2.714916
123.736691	2406.689767	5.737664	-0.024889	2.719110
124.047174	2414.700292	5.742669	-0.024952	2.723289
124.065426	2422.756295	5.747674	-0.024961	2.727468
124.456878	2430.803243	5.752678	-0.025040	2.731658
124.954561	2438.810284	5.757683	-0.025138	2.735828
125.222910	2446.860032	5.762688	-0.025193	2.739999
125.348860	2454.924501	5.767693	-0.025222	2.744163
125.711636	2462.930831	5.772698	-0.025296	2.748305
126.132130	2471.067314	5.777702	-0.025379	2.752511
126.336721	2479.129838	5.782707	-0.025423	2.756659
126.670177	2487.144965	5.787712	-0.025491	2.760785
126.965861	2495.158384	5.792717	-0.025551	2.764901
127.011849	2503.197866	5.797722	-0.025565	2.769010
127.249311	2511.266151	5.802726	-0.025615	2.773139
127.214148	2519.332402	5.807731	-0.025614	2.777244
127.542140	2527.351670	5.812736	-0.025681	2.781340
127.699853	2535.394146	5.817741	-0.025716	2.785433
127.989818	2543.420862	5.822746	-0.025775	2.789519
128.418885	2551.488450	5.827750	-0.025861	2.793628
128.684231	2559.490684	5.832755	-0.025916	2.797688
128.872460	2567.534657	5.837760	-0.025956	2.801759
129.340150	2575.547668	5.842765	-0.026049	2.805824
129.579437	2583.603839	5.847770	-0.026099	2.809892
129.682778	2591.705486	5.852774	-0.026124	2.813969
130.026452	2599.716649	5.857779	-0.026193	2.818009
130.321066	2607.740138	5.862784	-0.026254	2.822046
130.583841	2615.803284	5.867789	-0.026308	2.826095
130.759813	2623.834905	5.872794	-0.026347	2.830118
131.277164	2631.914925	5.877798	-0.026449	2.834178
131.754258	2639.883470	5.882803	-0.026543	2.838175
131.891857	2647.927832	5.887808	-0.026574	2.842184
132.143298	2655.984565	5.892813	-0.026627	2.846201
132.407399	2664.012973	5.897818	-0.026681	2.850198
132.743105	2672.088865	5.902822	-0.026749	2.854218
132.980869	2680.116011	5.907827	-0.026799	2.858202
133.025046	2688.171237	5.912832	-0.026813	2.862183
133.262684	2696.200763	5.917837	-0.026863	2.866157
133.540091	2704.226326	5.922842	-0.026920	2.870126
133.864673	2712.310588	5.927846	-0.026986	2.874120
134.025509	2720.325377	5.932851	-0.027021	2.878066
134.276609	2728.359655	5.937856	-0.027074	2.882021
134.560612	2736.420580	5.942861	-0.027132	2.885985
134.742351	2744.436432	5.947866	-0.027172	2.889917
135.063122	2752.493911	5.952870	-0.027237	2.893870
135.147643	2760.557403	5.957875	-0.027258	2.897809
135.501272	2768.561097	5.962880	-0.027330	2.901727
135.546369	2776.634294	5.967885	-0.027344	2.905658
135.738044	2784.640562	5.972890	-0.027385	2.909558
136.123491	2792.790242	5.977894	-0.027462	2.913533
136.319247	2800.787067	5.982899	-0.027504	2.917418
136.561257	2808.802505	5.987904	-0.027555	2.921310
137.061381	2816.785638	5.992909	-0.027653	2.925194
137.187261	2824.806321	5.997914	-0.027682	2.929072
137.512970	2832.882671	6.002918	-0.027749	2.932981
137.567515	2840.924869	6.007923	-0.027764	2.936855
137.729113	2848.950486	6.012928	-0.027800	2.940721
137.935091	2856.983245	6.017933	-0.027844	2.944588
138.072864	2865.026902	6.022938	-0.027875	2.948452
138.529724	2873.068874	6.027942	-0.027966	2.952326
138.694834	2881.112642	6.032947	-0.028002	2.956181
138.983531	2889.116399	6.037952	-0.028061	2.960018
139.420656	2897.123257	6.042957	-0.028148	2.963859
139.625738	2905.180080	6.047962	-0.028192	2.967706
139.881654	2913.253195	6.052966	-0.028245	2.971560
140.124483	2921.300190	6.057971	-0.028296	2.975395
140.130616	2929.334246	6.062976	-0.028303	2.979207
140.457809	2937.376036	6.067981	-0.028369	2.983034
140.483177	2945.412247	6.072986	-0.028379	2.986838
140.930746	2953.444304	6.077990	-0.028468	2.990656
141.227810	2961.497527	6.082995	-0.028529	2.994472
141.221795	2969.525650	6.088000	-0.028534	2.998256
141.529300	2977.533471	6.093005	-0.028596	3.002042
141.663118	2985.561901	6.098010	-0.028627	3.005824
142.365284	2993.556030	6.103014	-0.028763	3.009612
142.496971	3001.650485	6.108019	-0.028793	3.013415
142.519971	3009.693272	6.113024	-0.028803	3.017184
142.789413	3017.737715	6.118029	-0.028859	3.020961
143.038405	3025.734335	6.123034	-0.028911	3.024709
143.653167	3033.756445	6.128038	-0.029031	3.028483
143.727480	3041.835728	6.133043	-0.029050	3.032252
143.777688	3049.893386	6.138048	-0.029065	3.036005
144.232362	3057.875456	6.143053	-0.029155	3.039738
144.507624	3065.881430	6.148058	-0.029212	3.043469
144.818959	3073.944174	6.153062	-0.029275	3.047223
145.055763	3081.990990	6.158067	-0.029325	3.050962
145.302853	3090.040670	6.163072	-0.029377	3.054698
145.680011	3098.058592	6.168077	-0.029452	3.058420
145.762991	3106.086844	6.173082	-0.029473	3.062129
145.986124	3114.147145	6.178086	-0.029521	3.065855
146.212331	3122.164131	6.183091	-0.029568	3.069556
146.468213	3130.272820	6.188096	-0.029621	3.073297
146.903961	3138.299094	6.193101	-0.029708	3.077003
146.970412	3146.293073	6.198106	-0.029726	3.080673
147.496392	3154.269171	6.203110	-0.029830	3.084352
147.438055	3162.331892	6.208115	-0.029824	3.088039
147.809011	3170.381413	6.213120	-0.029899	3.091735
148.093298	3178.439913	6.218125	-0.029957	3.095427
148.029263	3186.446594	6.223130	-0.029951	3.099074
148.320318	3194.491540	6.228134	-0.030011	3.102751
148.501637	3202.518713	6.233139	-0.030050	3.106411
148.739525	3210.521610	6.238144	-0.030100	3.110058
149.040501	3218.591067	6.243149	-0.030161	3.113733
149.295993	3226.601692	6.248154	-0.030215	3.117376
149.503704	3234.648651	6.253158	-0.030259	3.121028
149.749890	3242.649523	6.258163	-0.030310	3.124657
150.042439	3250.675298	6.263168	-0.030370	3.128295
150.333738	3258.743932	6.268173	-0.030430	3.131948
150.362238	3266.802290	6.273178	-0.030441	3.135581
150.628008	3274.799478	6.278182	-0.030496	3.139192
150.778487	3282.835402	6.283187	-0.030529	3.142811
151.082921	3290.867676	6.288192	-0.030592	3.146432
151.171130	3298.921451	6.293197	-0.030614	3.150048
151.522903	3306.965087	6.298202	-0.030685	3.153667
151.731318	3314.997904	6.303206	-0.030729	3.157271
151.668984	3323.031385	6.308211	-0.030723	3.160859
151.953623	3331.011626	6.313216	-0.030782	3.164434
152.304042	3339.071724	6.318221	-0.030852	3.168044
152.384003	3347.094398	6.323226	-0.030873	3.171621
152.614074	3355.163656	6.328230	-0.030921	3.175221
152.982384	3363.157201	6.333235	-0.030995	3.178790
153.340023	3371.167981	6.338240	-0.031067	3.182361
153.462867	3379.225241	6.343245	-0.031096	3.185939
153.793477	3387.230148	6.348250	-0.031163	3.189499
154.040862	3395.322718	6.353254	-0.031215	3.193090
154.077523	3403.354832	6.358259	-0.031227	3.196641
154.563331	3411.326320	6.363264	-0.031323	3.200181
154.784385	3419.351831	6.368269	-0.031370	3.203729
154.978416	3427.366221	6.373274	-0.031411	3.207267
155.258138	3435.460278	6.378278	-0.031469	3.210840
155.448142	3443.487372	6.383283	-0.031510	3.214376
155.717004	3451.491794	6.388288	-0.031566	3.217901
155.903728	3459.539201	6.393293	-0.031606	3.221437
155.934670	3467.547392	6.398298	-0.031617	3.224946
156.444093	3475.594553	6.403302	-0.031718	3.228488
156.658310	3483.631182	6.408307	-0.031763	3.232010
156.801225	3491.717672	6.413312	-0.031795	3.235546
157.013538	3499.710658	6.418317	-0.031840	3.239040
157.267065	3507.702830	6.423322	-0.031893	3.242532
157.657724	3515.725518	6.428326	-0.031971	3.246039
158.105340	3523.702956	6.433331	-0.032060	3.249525
158.202470	3531.794136	6.438336	-0.032084	3.253042
158.379880	3539.852899	6.443341	-0.032122	3.256545
158.798785	3547.833394	6.448346	-0.032206	3.260019
159.165168	3555.849796	6.453350	-0.032280	3.263503
159.369523	3563.893365	6.458355	-0.032323	3.266989
159.683722	3571.931279	6.463360	-0.032387	3.270473
160.151419	3579.979894	6.468365	-0.032480	3.273964
160.305509	3587.994764	6.473370	-0.032514	3.277424
160.625824	3596.032882	6.478374	-0.032579	3.280897
160.588138	3604.041576	6.483379	-0.032578	3.284339
160.894603	3612.073437	6.488384	-0.032641	3.287802
161.215085	3620.142504	6.493389	-0.032706	3.291277
161.408066	3628.150098	6.498394	-0.032747	3.294717
161.896383	3636.164505	6.503398	-0.032844	3.298168
162.253755	3644.176618	6.508403	-0.032916	3.301609
162.399833	3652.205153	6.513408	-0.032949	3.305045
162.916222	3660.260386	6.518413	-0.033050	3.308503
163.203745	3668.296284	6.523418	-0.033109	3.311941
163.332903	3676.375976	6.528422	-0.033139	3.315388
163.547216	3684.358988	6.533427	-0.033184	3.318793
163.749940	3692.367498	6.538432	-0.033228	3.322205
163.956697	3700.409736	6.543437	-0.033272	3.325628
164.031698	3708.412297	6.548442	-0.033291	3.329025
164.341397	3716.474742	6.553446	-0.033355	3.332454
164.374306	3724.523366	6.558451	-0.033366	3.335862
164.444334	3732.520874	6.563456	-0.033385	3.339247
164.680835	3740.575629	6.568461	-0.033434	3.342659
164.865929	3748.579550	6.573466	-0.033474	3.346044
164.998146	3756.623667	6.578470	-0.033505	3.349440
165.335652	3764.664201	6.583475	-0.033573	3.352839
165.662536	3772.689482	6.588480	-0.033639	3.356228
165.827423	3780.714688	6.593485	-0.033676	3.359607
165.834521	3788.727395	6.598490	-0.033682	3.362972
166.268712	3796.760684	6.603494	-0.033769	3.366357
166.350483	3804.778738	6.608499	-0.033790	3.369720
166.439312	3812.816185	6.613504	-0.033812	3.373088
166.675471	3820.886520	6.618509	-0.033861	3.376472
166.960878	3828.853230	6.623514	-0.033920	3.379811
167.242431	3836.873189	6.628518	-0.033978	3.383168
167.340089	3844.918298	6.633523	-0.034002	3.386526
167.564540	3852.942757	6.638528	-0.034049	3.389877
167.917932	3861.066505	6.643533	-0.034120	3.393270
168.139222	3869.069893	6.648538	-0.034167	3.396605
168.433850	3877.055564	6.653542	-0.034227	3.399931
168.510904	3885.044042	6.658547	-0.034247	3.403249
168.652560	3893.071144	6.663552	-0.034279	3.406581
168.904401	3901.118139	6.668557	-0.034332	3.409922
169.174769	3909.126311	6.673562	-0.034388	3.413244
169.203323	3917.184353	6.678566	-0.034398	3.416575
169.520755	3925.178008	6.683571	-0.034463	3.419886
169.987900	3933.167234	6.688576	-0.034556	3.423197
170.426186	3941.209244	6.693581	-0.034643	3.426526
170.460669	3949.246109	6.698586	-0.034655	3.429836
170.707747	3957.295398	6.703590	-0.034706	3.433154
171.070740	3965.348464	6.708595	-0.034779	3.436475
171.226048	3973.314538	6.713600	-0.034814	3.439750
171.477766	3981.340630	6.718605	-0.034866	3.443050
171.718645	3989.364751	6.723610	-0.034917	3.446345
172.241786	3997.392177	6.728614	-0.035020	3.449648
172.286032	4005.465395	6.733619	-0.035033	3.452950
172.551686	4013.488036	6.738624	-0.035088	3.456236
172.750007	4021.523080	6.743629	-0.035131	3.459522
172.727949	4029.535237	6.748634	-0.035132	3.462788
173.027316	4037.585271	6.753638	-0.035194	3.466076
173.298218	4045.579353	6.758643	-0.035250	3.469338
173.298585	4053.651759	6.763648	-0.035255	3.472620
173.611483	4061.709346	6.768653	-0.035319	3.475903
174.048159	4069.642525	6.773658	-0.035406	3.479136
174.158643	4077.698395	6.778662	-0.035432	3.482405
174.040478	4085.721272	6.783667	-0.035416	3.485651
174.461273	4093.723177	6.788672	-0.035499	3.488902
175.074582	4101.748585	6.793677	-0.035619	3.492166
175.128658	4109.779058	6.798682	-0.035635	3.495411
175.223659	4117.849448	6.803686	-0.035658	3.498670
175.387293	4125.832203	6.808691	-0.035694	3.501894
175.563326	4133.850130	6.813696	-0.035732	3.505128
175.791555	4141.895581	6.818701	-0.035780	3.508373
175.865089	4149.917010	6.823706	-0.035800	3.511600
176.198583	4157.977192	6.828710	-0.035867	3.514847
176.274662	4165.967437	6.833715	-0.035887	3.518056
176.772388	4173.954566	6.838720	-0.035985	3.521273
176.991979	4181.997763	6.843725	-0.036032	3.524501
177.071050	4190.001378	6.848730	-0.036052	3.527706
177.367116	4198.059121	6.853734	-0.036113	3.530936
177.497129	4206.118980	6.858739	-0.036142	3.534159
177.538706	4214.153809	6.863744	-0.036156	3.537367
177.725136	4222.199144	6.868749	-0.036196	3.540580
177.939986	4230.163487	6.873754	-0.036241	3.543759
178.296501	4238.195889	6.878758	-0.036313	3.546966
178.328054	4246.261602	6.883763	-0.036325	3.550174
178.563691	4254.376026	6.888768	-0.036374	3.553404
178.836133	4262.409428	6.893773	-0.036431	3.556601
178.857188	4270.308144	6.898778	-0.036440	3.559733
179.127039	4278.325513	6.903782	-0.036496	3.562918
179.327131	4286.356122	6.908787	-0.036539	3.566102
179.625247	4294.352040	6.913792	-0.036600	3.569273
179.791724	4302.443140	6.918797	-0.036636	3.572474
179.758975	4310.444601	6.923802	-0.036636	3.575632
179.922607	4318.453835	6.928806	-0.036672	3.578795
180.323174	4326.452982	6.933811	-0.036752	3.581959
180.596223	4334.451198	6.938816	-0.036808	3.585116
180.790449	4342.499626	6.943821	-0.036850	3.588287
180.800720	4350.556638	6.948826	-0.036857	3.591454
180.976469	4358.592146	6.953830	-0.036896	3.594614
181.196913	4366.590200	6.958835	-0.036942	3.597757
181.358994	4374.585991	6.963840	-0.036978	3.600896
181.535963	4382.583788	6.968845	-0.037016	3.604033
181.765538	4390.600059	6.973850	-0.037065	3.607176
181.975807	4398.649573	6.978854	-0.037109	3.610329
182.171332	4406.704872	6.983859	-0.037151	3.613480
182.284799	4414.731480	6.988864	-0.037178	3.616616
182.626217	4422.736227	6.993869	-0.037247	3.619746
182.675912	4430.749329	6.998874	-0.037262	3.622869
182.954884	4438.784600	7.003878	-0.037319	3.626004
183.218554	4446.824012	7.008883	-0.037374	3.629138
183.449419	4454.887256	7.013888	-0.037423	3.632277
183.553304	4462.949518	7.018893	-0.037448	3.635409
183.529376	4470.874649	7.023898	-0.037449	3.638483
183.753453	4478.919896	7.028902	-0.037496	3.641607
184.069311	4486.925502	7.033907	-0.037560	3.644715
184.117341	4494.965381	7.038912	-0.037575	3.647827
184.284101	4503.042802	7.043917	-0.037611	3.650953
184.385890	4511.056459	7.048922	-0.037636	3.654051
184.663453	4519.041517	7.053926	-0.037693	3.657140
184.719480	4527.072005	7.058931	-0.037709	3.660237
184.971343	4535.060384	7.063936	-0.037761	3.663321
185.262927	4543.107299	7.068941	-0.037821	3.666426
185.379968	4551.134761	7.073946	-0.037849	3.669516
185.878851	4559.195422	7.078950	-0.037947	3.672626
185.895066	4567.234460	7.083955	-0.037956	3.675713
185.995781	4575.225774	7.088960	-0.037980	3.678781
186.506664	4583.237242	7.093965	-0.038081	3.681865
186.506664	4591.223519	7.098970	-0.038086	3.684923
186.578088	4599.271299	7.103974	-0.038105	3.688004
186.698737	4607.311979	7.108979	-0.038133	3.691081
187.026263	4615.322102	7.113984	-0.038199	3.694149
187.384267	4623.348495	7.118989	-0.038272	3.697221
187.246902	4631.340428	7.123994	-0.038252	3.700266
187.512821	4639.351108	7.128998	-0.038307	3.703325
187.819929	4647.405237	7.134003	-0.038369	3.706399
187.869342	4655.454169	7.139008	-0.038384	3.709462
188.187112	4663.553246	7.144013	-0.038449	3.712548
188.333415	4671.562522	7.149018	-0.038482	3.715593
188.765290	4679.538689	7.154022	-0.038568	3.718630
188.833826	4687.535790	7.159027	-0.038586	3.721664
188.776059	4695.495579	7.164032	-0.038581	3.724678
189.062578	4703.548794	7.169037	-0.038640	3.727733
189.175162	4711.580978	7.174042	-0.038666	3.730773
189.666062	4719.613188	7.179046	-0.038763	3.733820
189.606142	4727.667908	7.184051	-0.038757	3.736860
189.731543	4735.649629	7.189056	-0.038786	3.739875
189.870942	4743.670116	7.194061	-0.038818	3.742901
190.162290	4751.676058	7.199066	-0.038878	3.745924
190.274789	4759.736260	7.204070	-0.038904	3.748960
190.202387	4767.797928	7.209075	-0.038896	3.751990
190.587720	4775.774572	7.214080	-0.038973	3.754996
190.941772	4783.792161	7.219085	-0.039045	3.758014
190.949588	4791.809355	7.224090	-0.039052	3.761022
191.142869	4799.794938	7.229094	-0.039093	3.764020
191.359825	4807.872259	7.234099	-0.039139	3.767050
191.406733	4815.877251	7.239104	-0.039154	3.770047
191.708872	4823.947472	7.244109	-0.039216	3.773071
191.827503	4831.973564	7.249114	-0.039243	3.776073
192.115728	4839.932283	7.254118	-0.039302	3.779051
192.175089	4847.998257	7.259123	-0.039319	3.782061
192.385139	4855.979538	7.264128	-0.039364	3.785041
192.721088	4864.064506	7.269133	-0.039432	3.788059
192.806748	4872.090421	7.274138	-0.039453	3.791048
193.075564	4880.111838	7.279142	-0.039509	3.794037
192.942010	4888.145028	7.284147	-0.039490	3.797018
193.061044	4896.082091	7.289152	-0.039517	3.799968
193.360975	4904.120822	7.294157	-0.039579	3.802956
193.508873	4912.115946	7.299162	-0.039612	3.805923
193.745908	4920.134097	7.304166	-0.039661	3.808898
194.100836	4928.208307	7.309171	-0.039733	3.811894
193.996340	4936.214341	7.314176	-0.039719	3.814853
194.519282	4944.190266	7.319181	-0.039822	3.817811
194.584248	4952.237920	7.324186	-0.039840	3.820784
194.747221	4960.237147	7.329190	-0.039875	3.823738
195.110369	4968.313362	7.334195	-0.039949	3.826723
195.098393	4976.263134	7.339200	-0.039952	3.829651
195.429441	4984.397200	7.344205	-0.040019	3.832652
195.421038	4992.370201	7.349210	-0.040023	3.835584
195.596656	5000.379708	7.354214	-0.040061	3.838532
195.727712	5008.407319	7.359219	-0.040091	3.841482
195.989113	5016.361507	7.364224	-0.040145	3.844406
196.367211	5024.443976	7.369229	-0.040221	3.847378
196.432774	5032.407051	7.374234	-0.040239	3.850296
196.721429	5040.508858	7.379238	-0.040299	3.853268
196.747796	5048.577767	7.384243	-0.040309	3.856220
196.805058	5056.532408	7.389248	-0.040325	3.859129
197.167851	5064.597730	7.394253	-0.040398	3.862082
197.192816	5072.543251	7.399258	-0.040408	3.864983
197.431702	5080.597853	7.404262	-0.040458	3.867925
197.461507	5088.664916	7.409267	-0.040470	3.870865
197.799452	5096.905866	7.414272	-0.040538	3.873872
197.982942	5104.844100	7.419277	-0.040578	3.876764
198.047111	5112.749231	7.424282	-0.040595	3.879640
198.261460	5120.740765	7.429286	-0.040641	3.882547
198.772059	5128.717423	7.434291	-0.040741	3.885453
199.046517	5136.736077	7.439296	-0.040798	3.888367
199.183250	5144.814694	7.444301	-0.040829	3.891298
199.276814	5152.809483	7.449306	-0.040852	3.894195
199.654829	5160.866943	7.454310	-0.040928	3.897119
199.670572	5168.864967	7.459315	-0.040936	3.900012
199.626180	5176.835785	7.464320	-0.040934	3.902891
199.910243	5184.887078	7.469325	-0.040992	3.905804
200.007692	5192.894457	7.474330	-0.041016	3.908696
200.281546	5200.921231	7.479334	-0.041072	3.911595
200.364792	5208.996823	7.484339	-0.041093	3.914506
200.584178	5216.963935	7.489344	-0.041140	3.917379
200.955207	5225.003917	7.494349	-0.041214	3.920278
201.144936	5232.926313	7.499354	-0.041255	3.923130
201.307692	5240.980248	7.504358	-0.041291	3.926026
201.631316	5248.971193	7.509363	-0.041357	3.928901
201.818233	5257.030727	7.514368	-0.041397	3.931795
202.233134	5265.043927	7.519373	-0.041480	3.934675
202.172046	5273.099115	7.524378	-0.041474	3.937559
202.353892	5281.073086	7.529382	-0.041514	3.940416
202.628883	5289.089366	7.534387	-0.041570	3.943288
202.877198	5297.114676	7.539392	-0.041622	3.946161
203.134698	5305.142874	7.544397	-0.041676	3.949032
203.245162	5313.204347	7.549402	-0.041702	3.951911
203.226358	5321.229875	7.554406	-0.041704	3.954773
203.354746	5329.237429	7.559411	-0.041733	3.957628
203.466216	5337.220948	7.564416	-0.041759	3.960473
203.834176	5345.247079	7.569421	-0.041833	3.963335
203.951669	5353.231444	7.574426	-0.041861	3.966176
204.076830	5361.255507	7.579430	-0.041890	3.969030
204.184820	5369.327562	7.584435	-0.041915	3.971897
204.572255	5377.335948	7.589440	-0.041993	3.974745
204.706924	5385.375372	7.594445	-0.042024	3.977598
204.679876	5393.361224	7.599450	-0.042024	3.980427
205.134188	5401.371723	7.604454	-0.042114	3.983270
205.233228	5409.410857	7.609459	-0.042138	3.986116
205.054126	5417.411251	7.614464	-0.042110	3.988941
205.415018	5425.495768	7.619469	-0.042183	3.991803
205.608309	5433.538212	7.624474	-0.042225	3.994646
205.845532	5441.573841	7.629478	-0.042275	3.997484
206.050847	5449.556497	7.634483	-0.042318	4.000301
206.101117	5457.540382	7.639488	-0.042333	4.003115
206.153127	5465.588391	7.644493	-0.042348	4.005948
206.399710	5473.569452	7.649498	-0.042400	4.008760
206.585169	5481.626489	7.654502	-0.042440	4.011595
206.503935	5489.681642	7.659507	-0.042430	4.014423
206.570634	5497.679829	7.664512	-0.042448	4.017232
206.883333	5505.655860	7.669517	-0.042512	4.020034
206.982169	5513.686210	7.674522	-0.042536	4.022851
207.170135	5521.700500	7.679526	-0.042577	4.025661
207.307955	5529.753000	7.684531	-0.042608	4.028482
207.807450	5537.766043	7.689536	-0.042706	4.031292
208.107890	5545.898934	7.694541	-0.042768	4.034139
208.093278	5553.879585	7.699546	-0.042771	4.036927
208.362363	5561.824075	7.704550	-0.042826	4.039704
208.620328	5569.794324	7.709555	-0.042880	4.042487
208.505668	5577.788686	7.714560	-0.042864	4.045272
208.826243	5585.827513	7.719565	-0.042929	4.048077
208.773586	5593.876986	7.724570	-0.042925	4.050878
208.945363	5601.920827	7.729574	-0.042963	4.053679
209.047740	5609.949840	7.734579	-0.042987	4.056471
209.180427	5617.889672	7.739584	-0.043017	4.059231
209.600181	5625.967978	7.744589	-0.043101	4.062041
209.728816	5633.912761	7.749594	-0.043131	4.064799
209.990316	5642.010735	7.754598	-0.043185	4.067609
210.134662	5650.010100	7.759603	-0.043217	4.070382
210.153079	5658.030012	7.764608	-0.043226	4.073159
210.453686	5666.092793	7.769613	-0.043288	4.075952
210.627132	5674.019073	7.774618	-0.043325	4.078694
210.993756	5682.104888	7.779622	-0.043399	4.081492
211.202023	5690.067901	7.784627	-0.043444	4.084244
210.997979	5698.113331	7.789632	-0.043411	4.087017
211.234219	5706.107876	7.794637	-0.043461	4.089776
211.163988	5714.163435	7.799642	-0.043453	4.092550
211.535896	5722.161863	7.804646	-0.043528	4.095309
211.797885	5730.187354	7.809651	-0.043582	4.098073
211.766345	5738.191543	7.814656	-0.043582	4.100825
212.138144	5746.221085	7.819661	-0.043657	4.103588
212.441605	5754.254262	7.824666	-0.043719	4.106350
212.652988	5762.240041	7.829670	-0.043764	4.109093
212.813289	5770.321535	7.834675	-0.043799	4.111866
213.013702	5778.327753	7.839680	-0.043842	4.114612
213.383964	5786.362249	7.844685	-0.043916	4.117368
213.540097	5794.309852	7.849690	-0.043951	4.120089
213.676607	5802.354841	7.854694	-0.043982	4.122842
213.935599	5810.338616	7.859699	-0.044036	4.125573
213.889517	5818.358168	7.864704	-0.044033	4.128311
214.111605	5826.466617	7.869709	-0.044080	4.131081
214.115984	5834.470357	7.874714	-0.044086	4.133811
214.323884	5842.500474	7.879718	-0.044130	4.136550
214.584855	5850.510265	7.884723	-0.044184	4.139281
214.688890	5858.499855	7.889728	-0.044209	4.142002
215.022737	5866.504052	7.894733	-0.044277	4.144728
215.069982	5874.551328	7.899738	-0.044291	4.147464
215.250337	5882.584570	7.904742	-0.044330	4.150195
215.394332	5890.631813	7.909747	-0.044363	4.152928
215.399912	5898.636744	7.914752	-0.044369	4.155643
215.695023	5906.630497	7.919757	-0.044430	4.158357
216.024136	5914.677294	7.924762	-0.044497	4.161087
216.124564	5922.649675	7.929766	-0.044521	4.163787
216.285104	5930.677859	7.934771	-0.044556	4.166505
216.214822	5938.680339	7.939776	-0.044549	4.169210
216.754360	5946.735049	7.944781	-0.044655	4.171938
216.740536	5954.699918	7.949786	-0.044658	4.174627
217.076670	5962.769405	7.954790	-0.044726	4.177354
217.288720	5970.789122	7.959795	-0.044771	4.180060
217.372383	5978.783115	7.964800	-0.044792	4.182755
217.684190	5986.797146	7.969805	-0.044856	4.185458
217.801040	5994.800522	7.974810	-0.044883	4.188153
218.063260	6002.820224	7.979814	-0.044937	4.190853
218.219028	6010.984266	7.984819	-0.044972	4.193599
218.477164	6018.920838	7.989824	-0.045025	4.196267
218.824749	6026.899759	7.994829	-0.045096	4.198949
218.630066	6034.890684	7.999834	-0.045065	4.201628
219.088275	6042.828111	8.004838	-0.045156	4.204294
219.205388	6050.950976	8.009843	-0.045183	4.207017
219.393934	6058.882020	8.014848	-0.045224	4.209674
219.449787	6066.992082	8.019853	-0.045240	4.212388
219.496323	6074.994682	8.024858	-0.045254	4.215065
219.709874	6083.027262	8.029862	-0.045299	4.217751
219.835934	6091.026536	8.034867	-0.045328	4.220424
219.886752	6099.003238	8.039872	-0.045343	4.223087
220.264784	6107.070826	8.044877	-0.045419	4.225781
220.326673	6115.043398	8.049882	-0.045436	4.228440
220.401503	6123.098456	8.054886	-0.045456	4.231124
220.690895	6131.146817	8.059891	-0.045515	4.233806
220.827652	6139.158807	8.064896	-0.045546	4.236472
220.918694	6147.125555	8.069901	-0.045569	4.239122
220.849111	6155.167691	8.074906	-0.045561	4.241794
221.133058	6163.140003	8.079910	-0.045620	4.244444
221.453257	6171.196399	8.084915	-0.045685	4.247120
221.620416	6179.204831	8.089920	-0.045722	4.249777
221.874279	6187.247052	8.094925	-0.045774	4.252445
221.927861	6195.265044	8.099930	-0.045790	4.255101
222.045862	6203.298586	8.104934	-0.045817	4.257762
222.364853	6211.303449	8.109939	-0.045882	4.260413
222.419861	6219.295965	8.114944	-0.045898	4.263055
222.381139	6227.338506	8.119949	-0.045896	4.265712
222.476377	6235.386290	8.124954	-0.045920	4.268370
222.792034	6243.422937	8.129958	-0.045984	4.271025
222.986524	6251.489661	8.134963	-0.046026	4.273687
222.985100	6259.467073	8.139968	-0.046031	4.276316
223.382345	6267.449590	8.144973	-0.046111	4.278948
223.423440	6275.450067	8.149978	-0.046124	4.281582
223.532838	6283.456615	8.154982	-0.046150	4.284217
223.767425	6291.482100	8.159987	-0.046199	4.286857
223.908397	6299.479797	8.164992	-0.046231	4.289486
224.190238	6307.552223	8.169997	-0.046289	4.292138
224.429723	6315.592734	8.175002	-0.046339	4.294779
224.670280	6323.559228	8.180006	-0.046389	4.297393
224.695122	6331.554943	8.185011	-0.046399	4.300014
224.845894	6339.574469	8.190016	-0.046433	4.302641
225.108674	6347.583905	8.195021	-0.046487	4.305265
225.064682	6355.627522	8.200026	-0.046485	4.307896
225.216411	6363.658102	8.205030	-0.046519	4.310523
225.559886	6371.673916	8.210035	-0.046588	4.313144
225.614082	6379.718613	8.215040	-0.046604	4.315771
225.638199	6387.681837	8.220045	-0.046614	4.318370
225.691981	6395.687510	8.225050	-0.046629	4.320981
225.954753	6403.699127	8.230054	-0.046684	4.323594
226.603472	6411.742618	8.235059	-0.046810	4.326219
226.526896	6419.724708	8.240064	-0.046801	4.328817
226.953389	6427.801399	8.245069	-0.046886	4.331448
227.222771	6435.773232	8.250074	-0.046942	4.334041
227.156553	6443.827301	8.255078	-0.046935	4.336658
227.545579	6451.792893	8.260083	-0.047013	4.339247
227.727959	6459.831260	8.265088	-0.047053	4.341857
228.167140	6467.838387	8.270093	-0.047140	4.344457
228.221686	6475.872880	8.275098	-0.047156	4.347062
228.386762	6483.862727	8.280102	-0.047192	4.349651
228.480728	6491.974602	8.285107	-0.047215	4.352278
228.512822	6500.054055	8.290112	-0.047227	4.354893
228.765649	6508.032599	8.295117	-0.047279	4.357474
228.953573	6515.946714	8.300122	-0.047320	4.360033
229.101463	6523.959165	8.305126	-0.047353	4.362622
229.188387	6531.979552	8.310131	-0.047374	4.365211
229.329001	6539.974679	8.315136	-0.047406	4.367791
229.408084	6548.004817	8.320141	-0.047426	4.370380
229.619346	6556.062490	8.325146	-0.047471	4.372978
229.788187	6564.069582	8.330150	-0.047508	4.375557
230.097609	6572.061436	8.335155	-0.047571	4.378131
230.102592	6580.064603	8.340160	-0.047578	4.380705
230.288600	6588.107138	8.345165	-0.047618	4.383292
230.379676	6596.093971	8.350170	-0.047641	4.385858
230.577746	6604.080735	8.355174	-0.047683	4.388423
230.847063	6612.145967	8.360179	-0.047739	4.391013
230.948550	6620.197525	8.365184	-0.047763	4.393595
231.150182	6628.244380	8.370189	-0.047806	4.396175
231.004164	6636.193640	8.375194	-0.047785	4.398720
231.091403	6644.213839	8.380198	-0.047806	4.401288
231.393040	6652.206954	8.385203	-0.047868	4.403847
231.498930	6660.235354	8.390208	-0.047893	4.406415
231.750365	6668.252483	8.395213	-0.047946	4.408978
231.866329	6676.261853	8.400218	-0.047973	4.411536
231.827274	6684.332153	8.405222	-0.047971	4.414112
231.995251	6692.413769	8.410227	-0.048008	4.416691
232.124563	6700.314650	8.415232	-0.048037	4.419210
232.513618	6708.391654	8.420237	-0.048116	4.421785
232.455641	6716.351664	8.425242	-0.048110	4.424320
232.761168	6724.415918	8.430246	-0.048173	4.426888
233.100689	6732.460931	8.435251	-0.048241	4.429448
233.118523	6740.482889	8.440256	-0.048250	4.431998
233.245680	6748.535476	8.445261	-0.048280	4.434557
233.353896	6756.505496	8.450266	-0.048305	4.437088
233.386740	6764.460478	8.455270	-0.048317	4.439612
233.386426	6772.510060	8.460275	-0.048322	4.442165
233.542653	6780.460729	8.465280	-0.048357	4.444686
233.750043	6788.554317	8.470285	-0.048401	4.447251
233.958620	6796.533297	8.475290	-0.048445	4.449778
233.864632	6804.594751	8.480294	-0.048434	4.452328
234.102630	6812.626053	8.485299	-0.048483	4.454869
234.180344	6820.643256	8.490304	-0.048503	4.457403
234.394258	6828.631781	8.495309	-0.048549	4.459927
234.529292	6836.626850	8.500314	-0.048579	4.462451
234.627305	6844.622980	8.505318	-0.048603	4.464975
234.732080	6852.707783	8.510323	-0.048628	4.467524
234.900974	6860.669693	8.515328	-0.048665	4.470034
235.297520	6868.739719	8.520333	-0.048745	4.472577
235.364819	6876.768486	8.525338	-0.048763	4.475105
235.442924	6884.741161	8.530342	-0.048783	4.477613
235.781618	6892.730507	8.535347	-0.048851	4.480127
235.765035	6900.735099	8.540352	-0.048854	4.482642
235.719808	6908.757405	8.545357	-0.048851	4.485162
235.892322	6916.792996	8.550362	-0.048889	4.487684
236.051501	6924.813407	8.555366	-0.048924	4.490201
236.182956	6932.880484	8.560371	-0.048954	4.492731
236.304142	6940.797797	8.565376	-0.048982	4.495212
236.470600	6948.856729	8.570381	-0.049018	4.497737
236.620615	6956.875515	8.575386	-0.049052	4.500247
236.868603	6964.882016	8.580391	-0.049104	4.502752
236.948097	6972.884535	8.585395	-0.049124	4.505255
237.112094	6980.920818	8.590400	-0.049160	4.507766
237.392807	6988.963704	8.595405	-0.049218	4.510279
237.768734	6996.996428	8.600410	-0.049293	4.512787
237.838157	7005.002124	8.605415	-0.049312	4.515285
237.896001	7013.022392	8.610419	-0.049328	4.517786
237.891514	7020.969425	8.615424	-0.049333	4.520262
238.201496	7029.010813	8.620429	-0.049396	4.522767
238.212149	7036.958555	8.625434	-0.049404	4.525241
238.251675	7045.032930	8.630439	-0.049417	4.527753
238.612567	7053.042395	8.635443	-0.049489	4.530244
238.926584	7061.083854	8.640448	-0.049553	4.532743
238.862180	7069.106091	8.645453	-0.049547	4.535235
238.930379	7077.094700	8.650458	-0.049565	4.537715
239.259903	7085.084178	8.655463	-0.049632	4.540194
239.334168	7093.136000	8.660467	-0.049651	4.542690
239.250744	7101.098420	8.665472	-0.049641	4.545158
239.417453	7109.160626	8.670477	-0.049678	4.547655
239.576773	7117.193073	8.675482	-0.049713	4.550142
239.675097	7125.242395	8.680487	-0.049737	4.552632
240.016711	7133.280899	8.685491	-0.049806	4.555118
240.135008	7141.229945	8.690496	-0.049834	4.557575
240.241733	7149.221804	8.695501	-0.049859	4.560043
240.247617	7157.244756	8.700506	-0.049866	4.562520
240.381076	7165.248304	8.705511	-0.049896	4.564990
240.631140	7173.327719	8.710515	-0.049948	4.567481
240.719707	7181.290624	8.715520	-0.049970	4.569935
241.010401	7189.363637	8.720525	-0.050030	4.572422
240.823670	7197.350340	8.725530	-0.050001	4.574881
241.023273	7205.385823	8.730535	-0.050043	4.577354
241.289336	7213.377830	8.735539	-0.050098	4.579812
241.347637	7221.417439	8.740544	-0.050115	4.582283
241.594278	7229.419301	8.745549	-0.050166	4.584741
241.606770	7237.477935	8.750554	-0.050174	4.587215
241.920470	7245.459953	8.755559	-0.050238	4.589665
242.146190	7253.541216	8.760563	-0.050286	4.592143
242.208254	7261.538559	8.765568	-0.050303	4.594595
242.420936	7269.579757	8.770573	-0.050348	4.597058
242.371389	7277.466559	8.775578	-0.050344	4.599473
242.690850	7285.576533	8.780583	-0.050409	4.601955
242.774695	7293.541114	8.785587	-0.050430	4.604391
242.900877	7301.557942	8.790592	-0.050459	4.606842
243.072431	7309.583167	8.795597	-0.050497	4.609294
243.208570	7317.621951	8.800602	-0.050528	4.611749
243.364346	7325.619037	8.805607	-0.050562	4.614190
243.484131	7333.697199	8.810611	-0.050590	4.616654
243.554947	7341.611731	8.815616	-0.050609	4.619067
243.792772	7349.692458	8.820621	-0.050659	4.621529
243.906307	7357.669833	8.825626	-0.050685	4.623959
244.111260	7365.688479	8.830631	-0.050729	4.626399
244.285542	7373.675486	8.835635	-0.050767	4.628829
244.380818	7381.749844	8.840640	-0.050790	4.631284
244.659292	7389.818545	8.845645	-0.050848	4.633736
244.739693	7397.809039	8.850650	-0.050868	4.636163
245.065392	7405.731207	8.855655	-0.050935	4.638568
245.330321	7413.807751	8.860659	-0.050989	4.641019
245.185233	7421.798122	8.865664	-0.050968	4.643442
245.330113	7429.846933	8.870669	-0.051000	4.645882
245.387089	7437.793624	8.875674	-0.051017	4.648289
245.499828	7445.826106	8.880679	-0.051043	4.650721
245.682361	7453.933233	8.885683	-0.051083	4.653174
245.732827	7461.875989	8.890688	-0.051098	4.655577
245.995862	7469.902131	8.895693	-0.051152	4.658003
246.109069	7477.913407	8.900698	-0.051179	4.660423
246.327216	7485.912766	8.905703	-0.051225	4.662839
246.431484	7493.947971	8.910707	-0.051250	4.665264
246.510771	7501.927259	8.915712	-0.051270	4.667671
246.931469	7509.968168	8.920717	-0.051354	4.670095
247.298962	7518.045300	8.925722	-0.051428	4.672529
247.128746	7526.081659	8.930727	-0.051402	4.674949
247.448717	7534.105944	8.935731	-0.051467	4.677365
247.800971	7541.993530	8.940736	-0.051538	4.679737
247.842321	7550.025822	8.945741	-0.051551	4.682153
247.765248	7558.014864	8.950746	-0.051542	4.684554
247.864487	7566.042279	8.955751	-0.051566	4.686966
248.288419	7574.049841	8.960755	-0.051651	4.689369
248.358234	7582.070917	8.965760	-0.051669	4.691776
248.620380	7590.089058	8.970765	-0.051724	4.694181
248.611734	7598.168996	8.975770	-0.051728	4.696603
248.817412	7606.130556	8.980775	-0.051772	4.698988
248.949694	7614.163509	8.985779	-0.051802	4.701394
248.963257	7622.125708	8.990784	-0.051810	4.703777
249.057152	7630.205283	8.995789	-0.051833	4.706194
249.309516	7638.144058	9.000794	-0.051885	4.708568
249.546278	7646.221608	9.005799	-0.051935	4.710981
249.711811	7654.282968	9.010803	-0.051971	4.713389
249.644956	7662.242024	9.015808	-0.051964	4.715765
249.813842	7670.296005	9.020813	-0.052001	4.718168
249.984646	7678.273564	9.025818	-0.052039	4.720547
250.000213	7686.269571	9.030823	-0.052047	4.722931
250.321251	7694.333161	9.035827	-0.052113	4.725333
250.508105	7702.321110	9.040832	-0.052153	4.727711
250.835368	7710.350147	9.045837	-0.052219	4.730100
250.909453	7718.446038	9.050842	-0.052239	4.732508
250.994156	7726.375009	9.055847	-0.052260	4.734866
251.335141	7734.473387	9.060851	-0.052329	4.737272
251.232238	7742.402262	9.065856	-0.052315	4.739627
251.358127	7750.427871	9.070861	-0.052344	4.742010
251.501450	7758.419872	9.075866	-0.052377	4.744381
251.680398	7766.451062	9.080871	-0.052415	4.746762
251.746473	7774.499877	9.085875	-0.052433	4.749148
251.820090	7782.467489	9.090880	-0.052453	4.751509
252.182789	7790.552034	9.095885	-0.052526	4.753902
252.364924	7798.593358	9.100890	-0.052565	4.756281
252.468682	7806.527039	9.105895	-0.052590	4.758628
252.728276	7814.571089	9.110899	-0.052644	4.761006
252.793195	7822.553518	9.115904	-0.052661	4.763365
252.880832	7830.542331	9.120909	-0.052683	4.765724
253.066450	7838.583962	9.125914	-0.052723	4.768098
253.151538	7846.605126	9.130919	-0.052745	4.770465
253.427283	7854.675117	9.135923	-0.052802	4.772844
253.619322	7862.641172	9.140928	-0.052843	4.775192
253.704147	7870.699888	9.145933	-0.052864	4.777566
253.696105	7878.681882	9.150938	-0.052868	4.779917
253.770181	7886.630741	9.155943	-0.052888	4.782257
253.951806	7894.660375	9.160947	-0.052927	4.784618
253.949442	7902.674481	9.165952	-0.052932	4.786975
254.073043	7910.740020	9.170957	-0.052961	4.789345
254.363755	7918.770569	9.175962	-0.053020	4.791703
254.735087	7926.813817	9.180967	-0.053095	4.794064
254.688692	7934.773060	9.185971	-0.053092	4.796400
254.601750	7942.767501	9.190976	-0.053081	4.798745
254.992201	7950.834862	9.195981	-0.053160	4.801109
254.962209	7958.770946	9.200986	-0.053159	4.803435
254.998190	7966.802520	9.205991	-0.053172	4.805787
255.312392	7974.850978	9.210995	-0.053236	4.808142
255.254702	7982.818597	9.216000	-0.053231	4.810474
255.470066	7990.318317	9.221005	-0.053276	4.812667
255.672242	7994.834058	9.226010	-0.053317	4.813986

255.762231	7997.307997	9.231015	-0.053335	4.814709
255.817687	7998.675078	9.236019	-0.053347	4.815108
255.896107	7999.139988	9.241024	-0.053362	4.815244
256.413385	8000.223165	9.246029	-0.053460	4.815558
256.414631	8000.177276	9.251034	-0.053460	4.815544
256.401806	8000.147181	9.256039	-0.053458	4.815536
256.480909	8000.192308	9.261043	-0.053473	4.815548
256.456635	8000.154547	9.266048	-0.053469	4.815537
256.417860	8000.165689	9.271053	-0.053462	4.815541
256.590096	8000.196320	9.276058	-0.053494	4.815549
256.641909	8000.126690	9.281063	-0.053504	4.815528
256.776879	8000.183417	9.286067	-0.053530	4.815544
256.838378	8000.153474	9.291072	-0.053541	4.815535
256.791946	8000.211496	9.296077	-0.053533	4.815552
256.915572	8000.193256	9.301082	-0.053556	4.815547
256.923805	8000.201965	9.306087	-0.053558	4.815549
257.073015	8000.232219	9.311091	-0.053586	4.815557
257.085465	8000.188650	9.316096	-0.053589	4.815544
256.990022	8000.214887	9.321101	-0.053572	4.815552
257.009325	8000.197070	9.326106	-0.053575	4.815547
257.170308	8000.171965	9.331111	-0.053606	4.815539
257.145399	8000.196155	9.336115	-0.053601	4.815546
257.243562	8000.177497	9.341120	-0.053620	4.815540
257.498861	8000.219108	9.346125	-0.053668	4.815551
257.419039	8000.198595	9.351130	-0.053653	4.815546
257.173634	8000.143314	9.356135	-0.053608	4.815531
257.384930	8000.197023	9.361139	-0.053648	4.815545
257.284607	8000.210359	9.366144	-0.053629	4.815550
257.270453	8000.200540	9.371149	-0.053627	4.815547
257.330189	8000.195139	9.376154	-0.053638	4.815545
257.384772	8000.194994	9.381159	-0.053649	4.815545
257.620278	8000.233076	9.386163	-0.053693	4.815555
257.538180	8000.181544	9.391168	-0.053678	4.815540
257.657357	8000.214511	9.396173	-0.053701	4.815549
257.553636	8000.218177	9.401178	-0.053682	4.815551
257.478933	8000.202021	9.406183	-0.053668	4.815546
257.621320	8000.220412	9.411187	-0.053695	4.815551
257.521694	8000.214531	9.416192	-0.053677	4.815550
257.652139	8000.209223	9.421197	-0.053701	4.815547
257.669739	8000.168943	9.426202	-0.053705	4.815536
257.665143	8000.122957	9.431207	-0.053704	4.815522
257.902954	8000.198469	9.436211	-0.053749	4.815543
257.904039	8000.198514	9.441216	-0.053749	4.815543
257.946167	8000.201371	9.446221	-0.053757	4.815544
258.117853	8000.217039	9.451226	-0.053790	4.815547
257.987090	8000.214919	9.456231	-0.053766	4.815547
258.050332	8000.240557	9.461235	-0.053778	4.815555
258.078920	8000.219688	9.466240	-0.053783	4.815548
258.057731	8000.243939	9.471245	-0.053780	4.815556
257.884419	8000.189840	9.476250	-0.053748	4.815541
257.901780	8000.150625	9.481255	-0.053751	4.815529
257.790706	8000.211860	9.486259	-0.053731	4.815547
257.863914	8000.204543	9.491264	-0.053745	4.815545
257.985505	8000.236482	9.496269	-0.053768	4.815554
257.827638	8000.185841	9.501274	-0.053739	4.815540
258.000084	8000.171608	9.506279	-0.053771	4.815535
258.185655	8000.239853	9.511283	-0.053806	4.815554
258.239572	8000.205511	9.516288	-0.053817	4.815543
258.183499	8000.233463	9.521293	-0.053806	4.815552
258.317679	8000.208987	9.526298	-0.053832	4.815544
258.382744	8000.215425	9.531303	-0.053844	4.815546
258.450208	8000.210151	9.536307	-0.053857	4.815544
258.265625	8000.172960	9.541312	-0.053823	4.815534
258.271931	8000.208346	9.546317	-0.053824	4.815544
258.472291	8000.212734	9.551322	-0.053862	4.815544
258.204541	8000.231867	9.556327	-0.053813	4.815551
258.287102	8000.239661	9.561331	-0.053828	4.815553
258.168920	8000.235611	9.566336	-0.053807	4.815552
258.389265	8000.226438	9.571341	-0.053848	4.815549
258.201621	8000.203085	9.576346	-0.053813	4.815543
258.205033	8000.144410	9.581351	-0.053814	4.815526
258.521850	8000.237247	9.586355	-0.053874	4.815551
258.466159	8000.193626	9.591360	-0.053863	4.815539
258.501020	8000.251917	9.596365	-0.053870	4.815556
258.476525	8000.224834	9.601370	-0.053866	4.815548
258.329778	8000.208562	9.606375	-0.053839	4.815544
258.207794	8000.242909	9.611379	-0.053817	4.815554
258.186713	8000.198789	9.616384	-0.053813	4.815542
258.338957	8000.237641	9.621389	-0.053842	4.815552
258.243107	8000.215796	9.626394	-0.053824	4.815546
258.255048	8000.212815	9.631399	-0.053827	4.815545
258.567180	8000.199809	9.636403	-0.053885	4.815540
258.357335	8000.171817	9.641408	-0.053846	4.815533
258.360868	8000.221047	9.646413	-0.053847	4.815547
258.602713	8000.214365	9.651418	-0.053893	4.815544
258.333368	8000.209967	9.656423	-0.053843	4.815544
258.153355	8000.259386	9.661427	-0.053810	4.815559
258.194076	8000.207734	9.666432	-0.053818	4.815544
258.612671	8000.226391	9.671437	-0.053896	4.815547
258.421153	8000.201905	9.676442	-0.053860	4.815541
258.600485	8000.166419	9.681447	-0.053894	4.815530
258.778582	8000.229201	9.686451	-0.053928	4.815547
258.588640	8000.181237	9.691456	-0.053893	4.815534
258.617763	8000.187085	9.696461	-0.053898	4.815536
258.693404	8000.173399	9.701466	-0.053913	4.815532
258.671398	8000.183748	9.706471	-0.053909	4.815535
258.778087	8000.274203	9.711475	-0.053929	4.815561
258.652226	8000.248659	9.716480	-0.053906	4.815554
258.798082	8000.189118	9.721485	-0.053933	4.815536
258.877529	8000.173358	9.726490	-0.053949	4.815531
258.804110	8000.164701	9.731495	-0.053935	4.815528
258.897689	8000.265624	9.736499	-0.053953	4.815557
258.867098	8000.213868	9.741504	-0.053948	4.815542
258.799428	8000.239492	9.746509	-0.053935	4.815550
258.982787	8000.213688	9.751514	-0.053970	4.815542
258.828401	8000.164171	9.756519	-0.053941	4.815528
258.852757	8000.237247	9.761523	-0.053946	4.815549
258.720185	8000.212661	9.766528	-0.053922	4.815543
258.953812	8000.218665	9.771533	-0.053966	4.815543
258.886486	8000.168441	9.776538	-0.053953	4.815529
258.765026	8000.150448	9.781543	-0.053931	4.815524
258.866991	8000.220526	9.786547	-0.053950	4.815544
258.746055	8000.180106	9.791552	-0.053928	4.815533
258.789561	8000.208626	9.796557	-0.053937	4.815541
258.767162	8000.181577	9.801562	-0.053933	4.815533
258.870007	8000.172611	9.806567	-0.053952	4.815530
258.909852	8000.206413	9.811571	-0.053960	4.815540
258.843881	8000.195741	9.816576	-0.053948	4.815537
259.050132	8000.208774	9.821581	-0.053987	4.815540
258.963506	8000.230882	9.826586	-0.053971	4.815547
258.975526	8000.205466	9.831591	-0.053973	4.815539
259.174540	8000.250431	9.836595	-0.054011	4.815552
258.963793	8000.225628	9.841600	-0.053972	4.815545
259.039199	8000.226895	9.846605	-0.053986	4.815545
258.995749	8000.211252	9.851610	-0.053978	4.815541
259.132751	8000.203916	9.856615	-0.054004	4.815538
259.016287	8000.262926	9.861619	-0.053983	4.815556
258.897316	8000.215059	9.866624	-0.053961	4.815542
258.995273	8000.247680	9.871629	-0.053980	4.815552
259.287903	8000.237560	9.876634	-0.054034	4.815547
258.926839	8000.217765	9.881639	-0.053968	4.815543
259.056599	8000.220993	9.886643	-0.053992	4.815543
259.103839	8000.192952	9.891648	-0.054001	4.815535
259.113921	8000.257247	9.896653	-0.054003	4.815554
258.973203	8000.240005	9.901658	-0.053977	4.815549
259.107697	8000.230491	9.906663	-0.054003	4.815546
259.143025	8000.237510	9.911667	-0.054010	4.815548
259.229186	8000.197287	9.916672	-0.054026	4.815536
259.300325	8000.204895	9.921677	-0.054040	4.815537
259.244473	8000.222167	9.926682	-0.054029	4.815543
259.079860	8000.220557	9.931687	-0.053999	4.815543
259.401257	8000.254714	9.936691	-0.054059	4.815552
259.234477	8000.191103	9.941696	-0.054029	4.815534
259.282319	8000.192986	9.946701	-0.054038	4.815534
259.236407	8000.192259	9.951706	-0.054030	4.815534
259.203489	8000.161831	9.956711	-0.054024	4.815525
259.190371	8000.215062	9.961715	-0.054022	4.815541
259.235452	8000.212626	9.966720	-0.054030	4.815540
259.163878	8000.200793	9.971725	-0.054017	4.815537
259.269261	8000.200416	9.976730	-0.054037	4.815536
259.138673	8000.177999	9.981735	-0.054013	4.815530
259.150042	8000.241247	9.986739	-0.054016	4.815549
259.266472	8000.190839	9.991744	-0.054038	4.815533
259.520195	8000.240977	9.996749	-0.054085	4.815547
259.498983	8000.226767	10.001754	-0.054082	4.815543
259.368280	8000.244946	10.006759	-0.054058	4.815549
259.475570	8000.260626	10.011763	-0.054078	4.815553
259.319755	8000.177965	10.016768	-0.054049	4.815529
259.244705	8000.231246	10.021773	-0.054036	4.815545
259.287282	8000.247999	10.026778	-0.054044	4.815550
259.219608	8000.259735	10.031783	-0.054032	4.815554
259.366661	8000.247223	10.036787	-0.054059	4.815549
259.314847	8000.203664	10.041792	-0.054050	4.815537
259.380657	8000.236825	10.046797	-0.054062	4.815546
259.270305	8000.211534	10.051802	-0.054042	4.815539
259.378408	8000.212271	10.056807	-0.054063	4.815539
259.570337	8000.252847	10.061811	-0.054099	4.815550
259.367554	8000.228174	10.066816	-0.054061	4.815544
259.648504	8000.254188	10.071821	-0.054114	4.815550
259.448176	8000.239170	10.076826	-0.054077	4.815547
259.519323	8000.192290	10.081831	-0.054090	4.815532
259.554112	8000.218531	10.086835	-0.054097	4.815540
259.503979	8000.188888	10.091840	-0.054088	4.815532
259.685930	8000.235711	10.096845	-0.054122	4.815544
259.464840	8000.202190	10.101850	-0.054082	4.815536
259.398158	8000.147703	10.106855	-0.054069	4.815520
259.634011	8000.250967	10.111859	-0.054114	4.815549
259.522951	8000.233143	10.116864	-0.054093	4.815544
259.369386	8000.248809	10.121869	-0.054065	4.815550
259.485134	8000.258218	10.126874	-0.054087	4.815552
259.387521	8000.223521	10.131879	-0.054069	4.815542
259.437205	8000.298084	10.136883	-0.054079	4.815564
259.523268	8000.263202	10.141888	-0.054095	4.815553
259.447320	8000.296169	10.146893	-0.054081	4.815563
259.600077	8000.285888	10.151898	-0.054110	4.815559
259.616513	8000.218878	10.156903	-0.054113	4.815540
259.611558	8000.230576	10.161907	-0.054113	4.815543
259.515221	8000.212995	10.166912	-0.054095	4.815538
259.538701	8000.229434	10.171917	-0.054100	4.815543
259.555317	8000.223325	10.176922	-0.054103	4.815541
259.650074	8000.159739	10.181927	-0.054121	4.815522
259.657113	8000.217575	10.186931	-0.054123	4.815539
259.534205	8000.209172	10.191936	-0.054100	4.815537
259.743248	8000.240415	10.196941	-0.054139	4.815545
259.598884	8000.194265	10.201946	-0.054113	4.815532
259.576490	8000.188583	10.206951	-0.054109	4.815531
259.711676	8000.235706	10.211955	-0.054134	4.815544
259.547583	8000.212736	10.216960	-0.054104	4.815538
259.631431	8000.249399	10.221965	-0.054120	4.815548
259.685842	8000.253527	10.226970	-0.054131	4.815549
259.524896	8000.207105	10.231975	-0.054101	4.815537
259.787758	8000.258463	10.236979	-0.054150	4.815550
259.725769	8000.225420	10.241984	-0.054139	4.815541
259.592000	8000.243548	10.246989	-0.054114	4.815547
259.725136	8000.232944	10.251994	-0.054139	4.815543
259.621018	8000.200277	10.256999	-0.054120	4.815534
259.799291	8000.265202	10.262003	-0.054154	4.815552
259.737260	8000.228953	10.267008	-0.054143	4.815542
259.640396	8000.234867	10.272013	-0.054125	4.815544
259.796311	8000.242801	10.277018	-0.054154	4.815546
259.892629	8000.242275	10.282023	-0.054173	4.815545
259.726661	8000.260942	10.287027	-0.054142	4.815551
259.818664	8000.190900	10.292032	-0.054159	4.815530
259.961803	8000.218923	10.297037	-0.054186	4.815538
259.987409	8000.241808	10.302042	-0.054191	4.815544
259.798664	8000.233391	10.307047	-0.054157	4.815543
260.014308	8000.249785	10.312051	-0.054197	4.815547
259.795991	8000.224855	10.317056	-0.054157	4.815540
259.919371	8000.262169	10.322061	-0.054180	4.815551
259.955683	8000.249973	10.327066	-0.054187	4.815547
259.816712	8000.234895	10.332071	-0.054162	4.815543
259.951775	8000.249964	10.337075	-0.054187	4.815547
259.928120	8000.260287	10.342080	-0.054183	4.815550
260.029748	8000.269465	10.347085	-0.054202	4.815552
259.862152	8000.266737	10.352090	-0.054171	4.815552
259.960681	8000.270521	10.357095	-0.054190	4.815553
260.125182	8000.228381	10.362099	-0.054221	4.815540
259.942571	8000.218996	10.367104	-0.054187	4.815538
259.973393	8000.188547	10.372109	-0.054193	4.815529
259.839228	8000.245131	10.377114	-0.054169	4.815546
260.082956	8000.179720	10.382119	-0.054214	4.815526
259.925303	8000.225234	10.387123	-0.054185	4.815540
259.832907	8000.226948	10.392128	-0.054168	4.815541
259.905374	8000.274108	10.397133	-0.054182	4.815554
260.192020	8000.244661	10.402138	-0.054236	4.815544
259.905557	8000.213268	10.407143	-0.054183	4.815536
260.115262	8000.257343	10.412147	-0.054222	4.815548
260.050159	8000.208223	10.417152	-0.054210	4.815534
260.223489	8000.248495	10.422157	-0.054243	4.815545
260.186177	8000.260730	10.427162	-0.054236	4.815549
260.042243	8000.211381	10.432167	-0.054210	4.815535
260.009643	8000.262156	10.437171	-0.054204	4.815550
259.997357	8000.235272	10.442176	-0.054202	4.815542
260.179327	8000.261797	10.447181	-0.054236	4.815549
260.074094	8000.248342	10.452186	-0.054217	4.815546
260.037852	8000.201832	10.457191	-0.054211	4.815532
260.069928	8000.232303	10.462195	-0.054217	4.815541
259.981585	8000.161432	10.467200	-0.054201	4.815521
259.955635	8000.198427	10.472205	-0.054196	4.815532
260.101184	8000.219011	10.477210	-0.054224	4.815537
260.088460	8000.227377	10.482215	-0.054222	4.815539
260.130861	8000.271906	10.487219	-0.054230	4.815552
260.033401	8000.215843	10.492224	-0.054212	4.815536
260.103829	8000.254423	10.497229	-0.054225	4.815547
260.034954	8000.250113	10.502234	-0.054213	4.815546
260.051064	8000.231175	10.507239	-0.054216	4.815541
260.204196	8000.248678	10.512243	-0.054245	4.815545
260.141929	8000.182510	10.517248	-0.054234	4.815526
260.279938	8000.231816	10.522253	-0.054260	4.815540
260.333446	8000.224177	10.527258	-0.054270	4.815537
260.030671	8000.227773	10.532263	-0.054214	4.815540
260.079296	8000.245695	10.537267	-0.054223	4.815545
260.221989	8000.183965	10.542272	-0.054250	4.815526
260.170453	8000.218403	10.547277	-0.054241	4.815536
260.121199	8000.236852	10.552282	-0.054232	4.815542
259.956173	8000.210661	10.557287	-0.054202	4.815535
260.183131	8000.228310	10.562291	-0.054244	4.815539
260.176342	8000.210064	10.567296	-0.054243	4.815534
260.150306	8000.241715	10.572301	-0.054239	4.815543
260.270523	8000.261883	10.577306	-0.054262	4.815548
260.317086	8000.202846	10.582311	-0.054270	4.815531
260.307599	8000.221949	10.587315	-0.054269	4.815537
260.324731	8000.217985	10.592320	-0.054273	4.815535
260.301071	8000.236855	10.597325	-0.054268	4.815541
260.497922	8000.256146	10.602330	-0.054305	4.815546
260.355841	8000.231401	10.607335	-0.054279	4.815539
260.218495	8000.261222	10.612339	-0.054254	4.815548
260.276546	8000.257931	10.617344	-0.054265	4.815547
260.276007	8000.220556	10.622349	-0.054265	4.815536
260.215474	8000.235614	10.627354	-0.054254	4.815541
260.116172	8000.174179	10.632359	-0.054236	4.815523
260.238605	8000.227503	10.637363	-0.054259	4.815538
260.105398	8000.212519	10.642368	-0.054235	4.815535
260.339672	8000.258068	10.647373	-0.054279	4.815547
260.407926	8000.236781	10.652378	-0.054292	4.815540
260.321333	8000.189444	10.657383	-0.054276	4.815527
260.183901	8000.273752	10.662387	-0.054251	4.815552
260.287491	8000.246637	10.667392	-0.054270	4.815544
260.356859	8000.243532	10.672397	-0.054284	4.815542
260.323563	8000.246217	10.677402	-0.054278	4.815543
260.448544	8000.170307	10.682407	-0.054301	4.815521
260.449337	8000.238726	10.687411	-0.054302	4.815541
260.361694	8000.229833	10.692416	-0.054286	4.815538
260.426265	8000.212760	10.697421	-0.054298	4.815533
260.492640	8000.234179	10.702426	-0.054311	4.815539
260.347453	8000.228614	10.707431	-0.054284	4.815538
260.344545	8000.276672	10.712435	-0.054284	4.815552
260.410497	8000.231843	10.717440	-0.054296	4.815539
260.375090	8000.231289	10.722445	-0.054290	4.815539
260.247148	8000.231349	10.727450	-0.054267	4.815539
260.329451	8000.200679	10.732455	-0.054282	4.815530
260.445738	8000.243218	10.737459	-0.054304	4.815542
260.296143	8000.247196	10.742464	-0.054277	4.815544
260.446689	8000.240084	10.747469	-0.054305	4.815541
260.541300	8000.277994	10.752474	-0.054323	4.815552
260.276472	8000.233067	10.757479	-0.054274	4.815540
260.428750	8000.232394	10.762483	-0.054303	4.815539
260.589090	8000.196596	10.767488	-0.054333	4.815528
260.442810	8000.218792	10.772493	-0.054306	4.815535
260.252685	8000.275523	10.777498	-0.054271	4.815552
260.449003	8000.267028	10.782503	-0.054308	4.815549
260.440250	8000.271185	10.787507	-0.054306	4.815550
260.276328	8000.214028	10.792512	-0.054276	4.815534
260.291717	8000.199351	10.797517	-0.054279	4.815530
260.468654	8000.234341	10.802522	-0.054313	4.815539
260.419654	8000.172664	10.807527	-0.054304	4.815521
260.286492	8000.264522	10.812531	-0.054279	4.815549
260.346931	8000.230286	10.817536	-0.054291	4.815538
260.529504	8000.189512	10.822541	-0.054325	4.815526
260.682026	8000.246537	10.827546	-0.054354	4.815542
260.543796	8000.191939	10.832551	-0.054328	4.815526
260.572837	8000.266165	10.837555	-0.054334	4.815548
260.509291	8000.236301	10.842560	-0.054323	4.815539
260.689738	8000.286307	10.847565	-0.054357	4.815553
260.505001	8000.270475	10.852570	-0.054323	4.815549
260.459205	8000.229150	10.857575	-0.054314	4.815537
260.610076	8000.271191	10.862579	-0.054343	4.815549
260.566683	8000.246999	10.867584	-0.054335	4.815542
260.688708	8000.274676	10.872589	-0.054358	4.815550
260.520415	8000.291168	10.877594	-0.054327	4.815555
260.477983	8000.231735	10.882599	-0.054319	4.815538
260.716109	8000.262390	10.887603	-0.054364	4.815546
260.474454	8000.236006	10.892608	-0.054319	4.815539
260.437441	8000.274956	10.897613	-0.054313	4.815551
260.655548	8000.283914	10.902618	-0.054354	4.815552
260.825678	8000.265372	10.907623	-0.054386	4.815546
260.716594	8000.281768	10.912627	-0.054366	4.815552
260.509096	8000.257015	10.917632	-0.054327	4.815545
260.600695	8000.279918	10.922637	-0.054345	4.815552
260.545798	8000.279042	10.927642	-0.054335	4.815552
260.286954	8000.245966	10.932647	-0.054287	4.815543
260.524600	8000.271270	10.937651	-0.054332	4.815549
260.513350	8000.217692	10.942656	-0.054330	4.815534
260.496704	8000.291167	10.947661	-0.054327	4.815555
260.554000	8000.309232	10.952666	-0.054338	4.815560
260.428101	8000.242016	10.957671	-0.054315	4.815541
260.597486	8000.256582	10.962675	-0.054347	4.815545
260.388618	8000.241422	10.967680	-0.054308	4.815541
260.532143	8000.256631	10.972685	-0.054335	4.815545
260.406787	8000.273829	10.977690	-0.054312	4.815551
260.501122	8000.181388	10.982695	-0.054330	4.815523
260.705397	8000.287344	10.987699	-0.054368	4.815553
260.690315	8000.228360	10.992704	-0.054366	4.815536
260.567829	8000.248810	10.997709	-0.054343	4.815542
260.627487	8000.258367	11.002714	-0.054355	4.815545
260.756255	8000.275471	11.007719	-0.054379	4.815549
260.762939	8000.307661	11.012723	-0.054381	4.815559
260.511041	8000.258672	11.017728	-0.054334	4.815546
260.655756	8000.210864	11.022733	-0.054361	4.815531
260.712352	8000.241739	11.027738	-0.054372	4.815540
260.702232	8000.217026	11.032743	-0.054371	4.815532
260.611535	8000.264710	11.037747	-0.054354	4.815547
260.729941	8000.285917	11.042752	-0.054376	4.815552
260.458055	8000.273993	11.047757	-0.054326	4.815550
260.557917	8000.301306	11.052762	-0.054345	4.815558
260.525264	8000.187544	11.057767	-0.054339	4.815525
260.602585	8000.187776	11.062771	-0.054354	4.815524
260.525009	8000.206827	11.067776	-0.054340	4.815530
260.503786	8000.248174	11.072781	-0.054336	4.815542
260.824558	8000.228905	11.077786	-0.054396	4.815535
260.762868	8000.222576	11.082791	-0.054385	4.815534
260.764923	8000.312385	11.087795	-0.054386	4.815560
260.693985	8000.261030	11.092800	-0.054373	4.815545
260.674640	8000.267150	11.097805	-0.054370	4.815547
260.551384	8000.268356	11.102810	-0.054347	4.815548
260.497366	8000.270700	11.107815	-0.054337	4.815549
260.796676	8000.320525	11.112819	-0.054393	4.815562
260.628761	8000.266507	11.117824	-0.054362	4.815547
260.764865	8000.268773	11.122829	-0.054388	4.815547
260.880370	8000.295275	11.127834	-0.054410	4.815554
260.774695	8000.273264	11.132839	-0.054390	4.815548
260.431884	8000.285816	11.137843	-0.054327	4.815554
260.642027	8000.257248	11.142848	-0.054366	4.815544
260.604737	8000.278031	11.147853	-0.054360	4.815551
260.593270	8000.286418	11.152858	-0.054358	4.815553
260.581055	8000.254192	11.157863	-0.054356	4.815544
260.575288	8000.280835	11.162867	-0.054355	4.815552
260.586724	8000.250067	11.167872	-0.054358	4.815542
260.654476	8000.229841	11.172877	-0.054370	4.815536
260.819153	8000.204799	11.177882	-0.054401	4.815528
260.514188	8000.242547	11.182887	-0.054345	4.815541
260.775965	8000.282139	11.187891	-0.054394	4.815551
260.834055	8000.275643	11.192896	-0.054405	4.815549
260.733964	8000.290051	11.197901	-0.054387	4.815553
260.617204	8000.276405	11.202906	-0.054365	4.815550
260.710858	8000.258742	11.207911	-0.054383	4.815544
260.798965	8000.276246	11.212915	-0.054400	4.815549
260.712302	8000.271643	11.217920	-0.054384	4.815548
260.660918	8000.269757	11.222925	-0.054375	4.815548
260.904088	8000.296222	11.227930	-0.054420	4.815554
260.902995	8000.259905	11.232935	-0.054421	4.815544
260.831695	8000.274787	11.237939	-0.054408	4.815548
260.649331	8000.277157	11.242944	-0.054374	4.815550
260.691736	8000.223392	11.247949	-0.054382	4.815534
260.878549	8000.280983	11.252954	-0.054417	4.815550
260.825515	8000.249154	11.257959	-0.054408	4.815541
260.875173	8000.293804	11.262963	-0.054417	4.815554
260.720226	8000.239999	11.267968	-0.054389	4.815539
260.777151	8000.266605	11.272973	-0.054400	4.815546
260.787502	8000.283898	11.277978	-0.054402	4.815551
260.713904	8000.199378	11.282983	-0.054388	4.815527
260.732721	8000.283053	11.287987	-0.054392	4.815551
260.757843	8000.226867	11.292992	-0.054397	4.815535
260.920375	8000.260553	11.297997	-0.054428	4.815544
260.820026	8000.251451	11.303002	-0.054410	4.815542
260.514814	8000.210132	11.308007	-0.054353	4.815531
260.632962	8000.230266	11.313011	-0.054375	4.815536
260.738078	8000.238434	11.318016	-0.054395	4.815538
260.716372	8000.282978	11.323021	-0.054391	4.815551
260.913836	8000.306555	11.328026	-0.054429	4.815557
260.942817	8000.308128	11.333031	-0.054434	4.815557
260.848392	8000.313013	11.338035	-0.054417	4.815559
260.826948	8000.267814	11.343040	-0.054413	4.815546
260.758851	8000.280611	11.348045	-0.054401	4.815550
260.763222	8000.270027	11.353050	-0.054402	4.815547
260.891500	8000.247591	11.358055	-0.054426	4.815540
261.099828	8000.295920	11.363059	-0.054465	4.815553
260.773086	8000.283093	11.368064	-0.054405	4.815551
260.856384	8000.274876	11.373069	-0.054421	4.815548
260.896832	8000.263816	11.378074	-0.054429	4.815545
260.818147	8000.210197	11.383079	-0.054414	4.815529
260.849426	8000.281255	11.388083	-0.054420	4.815550
261.032534	8000.244764	11.393088	-0.054455	4.815538
261.065389	8000.277385	11.398093	-0.054461	4.815548
261.048391	8000.279270	11.403098	-0.054458	4.815548
260.781157	8000.255670	11.408103	-0.054409	4.815543
260.940381	8000.239085	11.413107	-0.054439	4.815537
260.790954	8000.269776	11.418112	-0.054411	4.815547
260.931855	8000.286012	11.423117	-0.054438	4.815551
260.775613	8000.295222	11.428122	-0.054409	4.815554
260.788266	8000.261268	11.433127	-0.054412	4.815544
260.826741	8000.289708	11.438131	-0.054419	4.815552
260.798336	8000.264695	11.443136	-0.054414	4.815545
260.721931	8000.278424	11.448141	-0.054400	4.815550
260.751095	8000.280000	11.453146	-0.054406	4.815550
260.837253	8000.240845	11.458151	-0.054422	4.815538
261.115250	8000.331989	11.463155	-0.054475	4.815563
260.832058	8000.271799	11.468160	-0.054422	4.815547
261.026258	8000.232285	11.473165	-0.054459	4.815535
260.977547	8000.282796	11.478170	-0.054450	4.815550
260.876098	8000.251239	11.483175	-0.054431	4.815541
261.010166	8000.333605	11.488179	-0.054457	4.815564
260.854414	8000.292606	11.493184	-0.054428	4.815553
261.070515	8000.245973	11.498189	-0.054468	4.815538
261.159674	8000.292342	11.503194	-0.054485	4.815552
260.974271	8000.242309	11.508199	-0.054451	4.815538
261.045055	8000.269143	11.513203	-0.054465	4.815545
261.122260	8000.250141	11.518208	-0.054479	4.815539
260.949570	8000.220617	11.523213	-0.054447	4.815532
260.968301	8000.291470	11.528218	-0.054451	4.815552
261.054211	8000.270474	11.533223	-0.054468	4.815546
261.228757	8000.315043	11.538227	-0.054500	4.815558
260.900870	8000.270144	11.543232	-0.054440	4.815546
260.798934	8000.250331	11.548237	-0.054421	4.815541
260.974785	8000.273552	11.553242	-0.054454	4.815547
260.931508	8000.283552	11.558247	-0.054446	4.815550
261.103093	8000.305635	11.563251	-0.054479	4.815556
261.080451	8000.258279	11.568256	-0.054475	4.815542
261.009394	8000.300944	11.573261	-0.054462	4.815555
261.223826	8000.289542	11.578266	-0.054502	4.815550
261.235008	8000.256632	11.583271	-0.054504	4.815541
261.223145	8000.333392	11.588275	-0.054503	4.815563
261.184650	8000.286844	11.593280	-0.054496	4.815550
261.183751	8000.292199	11.598285	-0.054496	4.815551
261.034792	8000.309008	11.603290	-0.054468	4.815557
260.779669	8000.275990	11.608295	-0.054421	4.815548
260.909489	8000.307002	11.613299	-0.054446	4.815557
260.852941	8000.283662	11.618304	-0.054436	4.815550
260.925947	8000.221854	11.623309	-0.054449	4.815532
260.903006	8000.259968	11.628314	-0.054445	4.815543
260.879447	8000.249992	11.633319	-0.054441	4.815540
261.041299	8000.261230	11.638323	-0.054472	4.815543
260.870604	8000.253107	11.643328	-0.054440	4.815541
260.955492	8000.284448	11.648333	-0.054456	4.815550
261.134955	8000.308797	11.653338	-0.054490	4.815556
260.986408	8000.260438	11.658343	-0.054463	4.815543
261.037241	8000.261302	11.663347	-0.054473	4.815543
261.004809	8000.241565	11.668352	-0.054467	4.815537
260.920152	8000.270116	11.673357	-0.054451	4.815546
260.942415	8000.267305	11.678362	-0.054456	4.815545
260.906372	8000.246439	11.683367	-0.054450	4.815539
260.943788	8000.248151	11.688371	-0.054457	4.815539
260.953248	8000.220556	11.693376	-0.054459	4.815531
261.097345	8000.177012	11.698381	-0.054486	4.815518
261.162572	8000.249698	11.703386	-0.054498	4.815539
260.776913	8000.228422	11.708391	-0.054427	4.815534
260.906258	8000.253015	11.713395	-0.054451	4.815541
260.906665	8000.244502	11.718400	-0.054452	4.815538
260.852636	8000.220136	11.723405	-0.054442	4.815532
260.879323	8000.248382	11.728410	-0.054447	4.815540
260.944766	8000.251623	11.733415	-0.054460	4.815540
261.094410	8000.277619	11.738419	-0.054488	4.815547
261.024722	8000.250858	11.743424	-0.054475	4.815540
260.978541	8000.252262	11.748429	-0.054467	4.815540
261.286847	8000.291553	11.753434	-0.054525	4.815550
261.197736	8000.230282	11.758439	-0.054508	4.815533
261.304021	8000.323945	11.763443	-0.054529	4.815560
261.162842	8000.258612	11.768448	-0.054503	4.815541
260.965886	8000.200909	11.773453	-0.054466	4.815525
261.090991	8000.284196	11.778458	-0.054490	4.815549
260.959419	8000.266032	11.783463	-0.054466	4.815544
261.290150	8000.283255	11.788467	-0.054528	4.815548
260.974560	8000.250311	11.793472	-0.054469	4.815540
260.832970	8000.212751	11.798477	-0.054443	4.815529
261.010382	8000.269119	11.803482	-0.054476	4.815545
261.004439	8000.226312	11.808487	-0.054476	4.815532
261.005303	8000.296870	11.813491	-0.054476	4.815553
261.058894	8000.243290	11.818496	-0.054486	4.815537
261.078923	8000.242579	11.823501	-0.054490	4.815537
261.059182	8000.302114	11.828506	-0.054487	4.815554
260.998285	8000.256266	11.833511	-0.054476	4.815541
261.109670	8000.262400	11.838515	-0.054497	4.815542
261.073982	8000.207351	11.843520	-0.054491	4.815527
261.049439	8000.261465	11.848525	-0.054487	4.815542
261.189828	8000.274487	11.853530	-0.054513	4.815546
261.133243	8000.254352	11.858535	-0.054503	4.815540
261.207106	8000.232089	11.863539	-0.054517	4.815533
261.054322	8000.256314	11.868544	-0.054489	4.815541
260.982985	8000.304316	11.873549	-0.054476	4.815555
261.095462	8000.297647	11.878554	-0.054497	4.815553
261.037069	8000.262524	11.883559	-0.054486	4.815543
261.241165	8000.300101	11.888563	-0.054525	4.815553
261.141534	8000.250409	11.893568	-0.054507	4.815539
261.075900	8000.285684	11.898573	-0.054495	4.815549
261.357863	8000.276462	11.903578	-0.054547	4.815545
261.070469	8000.234365	11.908583	-0.054494	4.815534
261.157233	8000.276422	11.913587	-0.054511	4.815546
261.226268	8000.226300	11.918592	-0.054524	4.815531
261.238551	8000.230804	11.923597	-0.054526	4.815532
261.163130	8000.270191	11.928602	-0.054513	4.815544
261.072694	8000.273005	11.933607	-0.054496	4.815546
261.381671	8000.285596	11.938611	-0.054554	4.815548
261.172227	8000.247987	11.943616	-0.054515	4.815538
261.144383	8000.279610	11.948621	-0.054511	4.815547
261.239365	8000.294022	11.953626	-0.054529	4.815551
261.217408	8000.245609	11.958631	-0.054525	4.815537
261.283817	8000.302289	11.963635	-0.054537	4.815553
261.334523	8000.279645	11.968640	-0.054547	4.815546
261.159943	8000.303511	11.973645	-0.054515	4.815554
261.175167	8000.320885	11.978650	-0.054518	4.815559
261.067954	8000.251837	11.983655	-0.054499	4.815539
261.228585	8000.327162	11.988659	-0.054529	4.815561
261.113809	8000.270810	11.993664	-0.054508	4.815545
261.086123	8000.205208	11.998669	-0.054503	4.815526
261.385455	8000.248625	12.003674	-0.054559	4.815537
261.480036	8000.227772	12.008679	-0.054577	4.815530
261.266057	8000.243510	12.013683	-0.054537	4.815536
261.245488	8000.247474	12.018688	-0.054534	4.815537
261.476911	8000.291911	12.023693	-0.054577	4.815549
261.519772	8000.332177	12.028698	-0.054586	4.815561
261.422949	8000.281462	12.033703	-0.054568	4.815546
261.315354	8000.283993	12.038707	-0.054548	4.815547
261.372489	8000.273209	12.043712	-0.054559	4.815544
261.260498	8000.311994	12.048717	-0.054538	4.815556
261.400785	8000.308989	12.053722	-0.054565	4.815554
261.195499	8000.243668	12.058727	-0.054527	4.815536
261.393659	8000.285421	12.063731	-0.054564	4.815547
261.348387	8000.266540	12.068736	-0.054556	4.815542
261.305072	8000.302183	12.073741	-0.054548	4.815553
261.462481	8000.325102	12.078746	-0.054578	4.815559
261.494636	8000.325659	12.083751	-0.054584	4.815559
261.387992	8000.318589	12.088755	-0.054565	4.815557
261.374994	8000.277802	12.093760	-0.054563	4.815545
261.223696	8000.214439	12.098765	-0.054535	4.815528
261.298683	8000.297971	12.103770	-0.054549	4.815552
261.250233	8000.266216	12.108775	-0.054540	4.815542
261.198142	8000.301714	12.113779	-0.054531	4.815553
261.042877	8000.286366	12.118784	-0.054502	4.815549
261.301163	8000.283165	12.123789	-0.054551	4.815547
261.408588	8000.320219	12.128794	-0.054571	4.815557
261.150111	8000.272187	12.133799	-0.054523	4.815545
261.399542	8000.306236	12.138803	-0.054570	4.815553
261.424699	8000.322705	12.143808	-0.054575	4.815558
261.477088	8000.312910	12.148813	-0.054585	4.815555
261.359861	8000.313146	12.153818	-0.054564	4.815556
261.361275	8000.293965	12.158823	-0.054564	4.815550
261.388965	8000.327570	12.163827	-0.054570	4.815560
261.324611	8000.304102	12.168832	-0.054558	4.815553
261.437347	8000.328422	12.173837	-0.054579	4.815560
261.325463	8000.343704	12.178842	-0.054559	4.815565
261.283862	8000.286419	12.183847	-0.054551	4.815548
261.506876	8000.293323	12.188851	-0.054593	4.815549
261.438509	8000.255898	12.193856	-0.054581	4.815538
261.155202	8000.258743	12.198861	-0.054528	4.815541
261.356266	8000.316570	12.203866	-0.054566	4.815557
261.314613	8000.266764	12.208871	-0.054559	4.815542
261.220622	8000.289820	12.213875	-0.054541	4.815549
261.220693	8000.280233	12.218880	-0.054542	4.815547
261.424470	8000.266519	12.223885	-0.054580	4.815542
261.470479	8000.298289	12.228890	-0.054589	4.815551
261.324199	8000.253171	12.233895	-0.054562	4.815538
261.493981	8000.311553	12.238899	-0.054594	4.815554
261.548867	8000.269746	12.243904	-0.054604	4.815542
261.281771	8000.251488	12.248909	-0.054555	4.815538
261.204243	8000.271609	12.253914	-0.054541	4.815544
261.248078	8000.228552	12.258919	-0.054549	4.815531
261.506442	8000.292665	12.263923	-0.054598	4.815549
261.418824	8000.306209	12.268928	-0.054582	4.815553
261.628294	8000.305411	12.273933	-0.054621	4.815552
261.537526	8000.321040	12.278938	-0.054605	4.815557
261.415403	8000.297689	12.283943	-0.054582	4.815551
261.557801	8000.290444	12.288947	-0.054609	4.815548
261.286492	8000.286007	12.293952	-0.054559	4.815548
261.224502	8000.215566	12.298957	-0.054547	4.815528
261.562613	8000.309839	12.303962	-0.054611	4.815553
261.398381	8000.259084	12.308967	-0.054581	4.815539
261.418470	8000.293632	12.313971	-0.054585	4.815549
261.133460	8000.274012	12.318976	-0.054532	4.815545
261.467555	8000.295564	12.323981	-0.054594	4.815550
261.466126	8000.295569	12.328986	-0.054594	4.815550
261.352442	8000.278767	12.333991	-0.054574	4.815545
261.401928	8000.335169	12.338995	-0.054583	4.815562
261.341608	8000.319246	12.344000	-0.054572	4.815557
261.348643	8000.295883	12.349005	-0.054574	4.815550
261.362797	8000.319650	12.354010	-0.054577	4.815557
261.269554	8000.278611	12.359015	-0.054560	4.815546
261.442498	8000.324223	12.364019	-0.054592	4.815558
261.331592	8000.292509	12.369024	-0.054572	4.815549
261.225816	8000.291864	12.374029	-0.054553	4.815550
261.583021	8000.327688	12.379034	-0.054619	4.815558
261.528535	8000.261643	12.384039	-0.054609	4.815539
261.415020	8000.308952	12.389043	-0.054589	4.815554
261.492510	8000.313460	12.394048	-0.054603	4.815555
261.325599	8000.302193	12.399053	-0.054573	4.815552
261.628134	8000.306132	12.404058	-0.054629	4.815552
261.513025	8000.247637	12.409063	-0.054608	4.815535
261.484261	8000.295272	12.414067	-0.054603	4.815549
261.300393	8000.270905	12.419072	-0.054569	4.815543
261.288750	8000.247235	12.424077	-0.054567	4.815536
261.609238	8000.279249	12.429082	-0.054627	4.815544
261.500273	8000.224061	12.434087	-0.054607	4.815528
261.500730	8000.276450	12.439091	-0.054608	4.815544
261.433980	8000.293543	12.444096	-0.054596	4.815549
261.450802	8000.251110	12.449101	-0.054599	4.815537
261.589892	8000.305781	12.454106	-0.054625	4.815552
261.313957	8000.260666	12.459111	-0.054574	4.815540
261.528752	8000.310173	12.464115	-0.054615	4.815553
261.491095	8000.263637	12.469120	-0.054608	4.815540
261.367820	8000.210351	12.474125	-0.054585	4.815525
261.667306	8000.262319	12.479130	-0.054641	4.815539
261.438263	8000.247893	12.484135	-0.054599	4.815536
261.502355	8000.285303	12.489139	-0.054611	4.815546
261.502149	8000.265027	12.494144	-0.054612	4.815540
261.586529	8000.299566	12.499149	-0.054628	4.815550
261.606064	8000.305257	12.504154	-0.054632	4.815552
261.489859	8000.260634	12.509159	-0.054610	4.815539
261.521688	8000.286829	12.514163	-0.054616	4.815547
261.461420	8000.278386	12.519168	-0.054606	4.815544
261.401178	8000.284901	12.524173	-0.054595	4.815547
261.553452	8000.315215	12.529178	-0.054623	4.815555
261.456475	8000.285867	12.534183	-0.054606	4.815547
261.551929	8000.315246	12.539187	-0.054624	4.815555
261.617076	8000.313141	12.544192	-0.054636	4.815554
261.662161	8000.309637	12.549197	-0.054645	4.815552
261.602215	8000.321499	12.554202	-0.054634	4.815556
261.461272	8000.293564	12.559207	-0.054608	4.815549
261.276045	8000.283065	12.564211	-0.054574	4.815547
261.554902	8000.278066	12.569216	-0.054626	4.815544
261.429464	8000.251455	12.574221	-0.054603	4.815537
261.539012	8000.310982	12.579226	-0.054624	4.815553
261.414090	8000.271558	12.584231	-0.054601	4.815542
261.471423	8000.293899	12.589235	-0.054612	4.815549
261.610031	8000.284455	12.594240	-0.054638	4.815545
261.661365	8000.261822	12.599245	-0.054648	4.815538
261.569152	8000.323371	12.604250	-0.054631	4.815557
261.540047	8000.326125	12.609255	-0.054626	4.815558
261.468780	8000.346349	12.614259	-0.054613	4.815564
261.431854	8000.308373	12.619264	-0.054606	4.815553
261.306404	8000.314883	12.624269	-0.054583	4.815556
261.528478	8000.335662	12.629274	-0.054625	4.815561
261.406827	8000.289881	12.634279	-0.054603	4.815548
261.529312	8000.298335	12.639283	-0.054626	4.815550
261.348097	8000.279354	12.644288	-0.054592	4.815545
261.487082	8000.259231	12.649293	-0.054618	4.815538
261.547518	8000.300855	12.654298	-0.054630	4.815550
261.429823	8000.255139	12.659303	-0.054608	4.815537
261.598205	8000.264349	12.664307	-0.054640	4.815539
261.821087	8000.308648	12.669312	-0.054682	4.815551
261.637911	8000.273606	12.674317	-0.054648	4.815542
261.803060	8000.323365	12.679322	-0.054679	4.815556
261.820600	8000.292696	12.684327	-0.054683	4.815547
261.775508	8000.289845	12.689331	-0.054675	4.815546
261.685630	8000.305488	12.694336	-0.054658	4.815551
261.525425	8000.309290	12.699341	-0.054629	4.815553
261.579719	8000.294185	12.704346	-0.054639	4.815548
261.436523	8000.228817	12.709351	-0.054613	4.815530
261.562848	8000.248019	12.714355	-0.054637	4.815535
261.559308	8000.297138	12.719360	-0.054636	4.815549
261.492281	8000.258666	12.724365	-0.054624	4.815538
261.684973	8000.298193	12.729370	-0.054660	4.815549
261.726985	8000.281817	12.734375	-0.054668	4.815544
261.628597	8000.296253	12.739379	-0.054651	4.815548
261.457468	8000.284916	12.744384	-0.054619	4.815546
261.612792	8000.267200	12.749389	-0.054648	4.815540
261.733863	8000.313027	12.754394	-0.054671	4.815553
261.563520	8000.286745	12.759399	-0.054640	4.815546
261.441854	8000.327509	12.764403	-0.054617	4.815558
261.650683	8000.307468	12.769408	-0.054657	4.815552
261.529635	8000.276655	12.774413	-0.054634	4.815543
261.659470	8000.288436	12.779418	-0.054659	4.815546
261.548597	8000.247106	12.784423	-0.054638	4.815534
261.731399	8000.320661	12.789427	-0.054673	4.815555
261.513759	8000.274368	12.794432	-0.054633	4.815542
261.527194	8000.278891	12.799437	-0.054635	4.815544
261.699505	8000.325562	12.804442	-0.054668	4.815557
261.719033	8000.310953	12.809447	-0.054672	4.815552
261.571713	8000.308555	12.814451	-0.054645	4.815552
261.681668	8000.311462	12.819456	-0.054665	4.815552
261.440702	8000.282949	12.824461	-0.054621	4.815545
261.513349	8000.316226	12.829466	-0.054635	4.815555
261.614386	8000.292274	12.834471	-0.054654	4.815547
261.667248	8000.312404	12.839475	-0.054664	4.815553
261.495726	8000.301061	12.844480	-0.054632	4.815550
261.697560	8000.250988	12.849485	-0.054670	4.815535
261.940154	8000.292406	12.854490	-0.054716	4.815546
261.699420	8000.287402	12.859495	-0.054671	4.815545
261.475216	8000.282671	12.864499	-0.054630	4.815545
261.459603	8000.308085	12.869504	-0.054627	4.815552
261.591316	8000.307075	12.874509	-0.054652	4.815552
261.586612	8000.321984	12.879514	-0.054652	4.815556
261.610196	8000.301031	12.884519	-0.054656	4.815550
261.658039	8000.332832	12.889523	-0.054665	4.815559
261.609953	8000.354506	12.894528	-0.054657	4.815565
261.553902	8000.323694	12.899533	-0.054647	4.815557
261.712090	8000.318847	12.904538	-0.054676	4.815554
261.577363	8000.266439	12.909543	-0.054652	4.815540
261.538434	8000.313907	12.914547	-0.054645	4.815554
261.786200	8000.329767	12.919552	-0.054691	4.815557
261.696925	8000.308024	12.924557	-0.054675	4.815551
261.810794	8000.300310	12.929562	-0.054696	4.815548
261.605565	8000.293754	12.934567	-0.054658	4.815547
261.582799	8000.296613	12.939571	-0.054655	4.815548
261.432654	8000.315538	12.944576	-0.054627	4.815555
261.525690	8000.302139	12.949581	-0.054645	4.815550
261.750335	8000.299454	12.954586	-0.054687	4.815548
261.570426	8000.266603	12.959591	-0.054654	4.815540
261.688753	8000.257894	12.964595	-0.054676	4.815537
261.746895	8000.281317	12.969600	-0.054687	4.815543
261.708883	8000.291404	12.974605	-0.054680	4.815546
261.701338	8000.301992	12.979610	-0.054679	4.815549
261.511994	8000.262576	12.984615	-0.054644	4.815539
261.760576	8000.307297	12.989619	-0.054691	4.815551
261.802996	8000.301612	12.994624	-0.054699	4.815549
261.742290	8000.231191	12.999629	-0.054688	4.815528
261.950360	8000.308368	13.004634	-0.054727	4.815550
261.745920	8000.263360	13.009639	-0.054689	4.815538
261.678463	8000.287920	13.014643	-0.054677	4.815545
261.459487	8000.264043	13.019648	-0.054637	4.815539
261.453682	8000.204142	13.024653	-0.054636	4.815522
261.457144	8000.258718	13.029658	-0.054637	4.815538
261.493224	8000.252929	13.034663	-0.054644	4.815536
261.659458	8000.292021	13.039667	-0.054675	4.815547
261.596083	8000.265362	13.044672	-0.054664	4.815539
261.499522	8000.267006	13.049677	-0.054646	4.815540
261.708333	8000.304662	13.054682	-0.054685	4.815550
261.884566	8000.286222	13.059687	-0.054718	4.815544
261.796758	8000.316858	13.064691	-0.054702	4.815553
261.715835	8000.288842	13.069696	-0.054688	4.815545
261.811278	8000.276551	13.074701	-0.054706	4.815541
261.739173	8000.289282	13.079706	-0.054693	4.815545
261.609827	8000.256195	13.084711	-0.054669	4.815536
261.607005	8000.287162	13.089715	-0.054669	4.815545
261.963795	8000.299474	13.094720	-0.054735	4.815547
261.795955	8000.336272	13.099725	-0.054704	4.815559
261.877262	8000.328023	13.104730	-0.054720	4.815556
261.881457	8000.285381	13.109735	-0.054721	4.815543
261.898152	8000.339107	13.114739	-0.054724	4.815559
261.755562	8000.302596	13.119744	-0.054698	4.815549
261.805882	8000.300247	13.124749	-0.054708	4.815548
261.803727	8000.342978	13.129754	-0.054708	4.815561
261.546837	8000.298175	13.134759	-0.054660	4.815549
261.795729	8000.321533	13.139763	-0.054707	4.815554
261.765546	8000.317858	13.144768	-0.054702	4.815553
261.642563	8000.248548	13.149773	-0.054679	4.815534
261.947696	8000.326255	13.154778	-0.054736	4.815555
261.982619	8000.284119	13.159783	-0.054743	4.815542
261.773565	8000.277500	13.164787	-0.054704	4.815542
261.746290	8000.258915	13.169792	-0.054699	4.815536
262.068956	8000.267460	13.174797	-0.054760	4.815537
262.012610	8000.283656	13.179802	-0.054750	4.815542
261.829341	8000.282803	13.184807	-0.054716	4.815543
261.916486	8000.343032	13.189811	-0.054732	4.815560
262.019069	8000.326585	13.194816	-0.054752	4.815555
261.851124	8000.288588	13.199821	-0.054721	4.815544
261.815695	8000.354278	13.204826	-0.054715	4.815564
261.786613	8000.328183	13.209831	-0.054710	4.815556
261.848538	8000.318546	13.214835	-0.054721	4.815553
261.867145	8000.297511	13.219840	-0.054725	4.815547
261.746819	8000.292352	13.224845	-0.054703	4.815546
261.761444	8000.323607	13.229850	-0.054706	4.815555
261.744300	8000.307325	13.234855	-0.054703	4.815550
261.854423	8000.329467	13.239859	-0.054724	4.815556
261.952830	8000.316156	13.244864	-0.054743	4.815552
261.582863	8000.280176	13.249869	-0.054674	4.815543
261.815685	8000.321434	13.254874	-0.054718	4.815554
261.919649	8000.284708	13.259879	-0.054737	4.815543
261.710635	8000.333650	13.264883	-0.054699	4.815558
261.601110	8000.341491	13.269888	-0.054679	4.815561
261.626494	8000.270349	13.274893	-0.054684	4.815540
261.889971	8000.311043	13.279898	-0.054733	4.815551
261.691118	8000.316344	13.284903	-0.054696	4.815553
261.619615	8000.299168	13.289907	-0.054683	4.815548
261.721131	8000.310483	13.294912	-0.054703	4.815551
261.745004	8000.274576	13.299917	-0.054707	4.815541
261.752077	8000.322802	13.304922	-0.054709	4.815555
261.743926	8000.304531	13.309927	-0.054708	4.815549
261.654497	8000.326593	13.314931	-0.054692	4.815556
261.762390	8000.327329	13.319936	-0.054712	4.815556
261.794432	8000.344980	13.324941	-0.054718	4.815561
261.945981	8000.305832	13.329946	-0.054747	4.815549
261.743135	8000.254440	13.334951	-0.054709	4.815535
261.767580	8000.286924	13.339955	-0.054714	4.815544
261.841354	8000.290303	13.344960	-0.054728	4.815545
261.797328	8000.259689	13.349965	-0.054720	4.815536
261.719149	8000.323607	13.354970	-0.054706	4.815555
261.685074	8000.279266	13.359975	-0.054700	4.815542
261.844687	8000.293675	13.364979	-0.054730	4.815546
261.620566	8000.302835	13.369984	-0.054689	4.815549
261.513544	8000.276526	13.374989	-0.054669	4.815542
261.824796	8000.327622	13.379994	-0.054727	4.815556
261.643573	8000.295818	13.384999	-0.054694	4.815547
261.658138	8000.314249	13.390003	-0.054697	4.815552
261.806566	8000.298557	13.395008	-0.054725	4.815547
261.818859	8000.307335	13.400013	-0.054728	4.815550
261.772176	8000.324758	13.405018	-0.054719	4.815555
261.719041	8000.269419	13.410023	-0.054710	4.815539
261.806565	8000.333928	13.415027	-0.054726	4.815557
261.791557	8000.313408	13.420032	-0.054724	4.815552
261.816040	8000.327729	13.425037	-0.054729	4.815556
261.932241	8000.327533	13.430042	-0.054751	4.815555
261.980219	8000.268516	13.435047	-0.054760	4.815537
261.964788	8000.256537	13.440051	-0.054757	4.815534
261.833793	8000.290736	13.445056	-0.054733	4.815545
261.842692	8000.318691	13.450061	-0.054735	4.815553
261.796720	8000.342536	13.455066	-0.054727	4.815560
261.808759	8000.289339	13.460071	-0.054729	4.815544
261.986437	8000.307251	13.465075	-0.054763	4.815549
262.089611	8000.308977	13.470080	-0.054782	4.815549
261.781057	8000.286829	13.475085	-0.054725	4.815544
261.936494	8000.341772	13.480090	-0.054754	4.815559
261.861155	8000.282861	13.485095	-0.054741	4.815542
261.849662	8000.291248	13.490099	-0.054739	4.815545
261.782909	8000.309409	13.495104	-0.054727	4.815550
261.849520	8000.293438	13.500109	-0.054740	4.815545
261.879298	8000.336695	13.505114	-0.054745	4.815558
261.747041	8000.244794	13.510119	-0.054721	4.815532
262.007987	8000.244844	13.515123	-0.054770	4.815530
261.976816	8000.306330	13.520128	-0.054764	4.815548
261.836944	8000.286960	13.525133	-0.054739	4.815543
262.038951	8000.322368	13.530138	-0.054777	4.815553
261.795788	8000.240394	13.535143	-0.054732	4.815530
261.920193	8000.336495	13.540147	-0.054755	4.815557
261.758719	8000.321043	13.545152	-0.054725	4.815554
261.763318	8000.267723	13.550157	-0.054727	4.815538
261.763861	8000.325457	13.555162	-0.054727	4.815555
261.769579	8000.266813	13.560167	-0.054728	4.815538
261.856616	8000.283232	13.565171	-0.054745	4.815542
261.846515	8000.253177	13.570176	-0.054743	4.815533
261.768044	8000.235886	13.575181	-0.054729	4.815529
261.845249	8000.314115	13.580186	-0.054744	4.815551
261.914854	8000.281097	13.585191	-0.054757	4.815541
261.831690	8000.294714	13.590195	-0.054742	4.815546
261.839901	8000.302357	13.595200	-0.054744	4.815548
261.689261	8000.305247	13.600205	-0.054716	4.815549
261.869851	8000.322138	13.605210	-0.054750	4.815553
261.877567	8000.291307	13.610215	-0.054752	4.815544
261.959155	8000.285199	13.615219	-0.054767	4.815542
262.082448	8000.324654	13.620224	-0.054790	4.815553
261.954660	8000.243510	13.625229	-0.054767	4.815530
262.022390	8000.304488	13.630234	-0.054780	4.815547
261.922868	8000.298603	13.635239	-0.054762	4.815546
261.762049	8000.290641	13.640243	-0.054732	4.815545
261.962784	8000.352740	13.645248	-0.054770	4.815562
262.005848	8000.342792	13.650253	-0.054778	4.815559
261.841578	8000.347595	13.655258	-0.054748	4.815561
261.710631	8000.285632	13.660263	-0.054724	4.815543
261.887400	8000.293913	13.665267	-0.054757	4.815545
261.994365	8000.305318	13.670272	-0.054777	4.815548
261.731595	8000.241185	13.675277	-0.054729	4.815530
262.066574	8000.317247	13.680282	-0.054791	4.815551
262.084855	8000.276974	13.685287	-0.054795	4.815539
261.847845	8000.270963	13.690291	-0.054751	4.815538
261.902727	8000.297537	13.695296	-0.054762	4.815546
261.880141	8000.256591	13.700301	-0.054758	4.815534
261.985202	8000.325663	13.705306	-0.054778	4.815554
261.783987	8000.287118	13.710311	-0.054741	4.815543
261.958600	8000.297500	13.715315	-0.054773	4.815546
262.099183	8000.277405	13.720320	-0.054800	4.815539
261.794454	8000.285237	13.725325	-0.054743	4.815543
262.077443	8000.297404	13.730330	-0.054796	4.815545
262.054446	8000.284231	13.735335	-0.054792	4.815541
262.113029	8000.308730	13.740339	-0.054804	4.815548
262.113010	8000.317306	13.745344	-0.054804	4.815551
262.072446	8000.278200	13.750349	-0.054797	4.815539
262.098849	8000.320334	13.755354	-0.054802	4.815552
261.716019	8000.284141	13.760359	-0.054731	4.815543
261.897634	8000.307460	13.765363	-0.054765	4.815549
261.963276	8000.328870	13.770368	-0.054778	4.815555
261.850464	8000.272548	13.775373	-0.054757	4.815539
261.740445	8000.301750	13.780378	-0.054737	4.815548
261.833279	8000.263773	13.785383	-0.054754	4.815536
261.862626	8000.257873	13.790387	-0.054760	4.815534
261.868722	8000.270823	13.795392	-0.054762	4.815538
262.054237	8000.287795	13.800397	-0.054797	4.815542
261.995743	8000.333873	13.805402	-0.054786	4.815556
261.979688	8000.298377	13.810407	-0.054783	4.815546
262.046314	8000.300570	13.815411	-0.054796	4.815546
261.946204	8000.290402	13.820416	-0.054778	4.815543
261.982176	8000.263242	13.825421	-0.054785	4.815535
262.124095	8000.280565	13.830426	-0.054811	4.815540
261.992059	8000.290172	13.835431	-0.054787	4.815543
262.023454	8000.298196	13.840435	-0.054793	4.815545
262.117470	8000.319005	13.845440	-0.054811	4.815551
261.918857	8000.338200	13.850445	-0.054775	4.815557
262.148169	8000.349484	13.855450	-0.054818	4.815560
261.916618	8000.310439	13.860455	-0.054775	4.815549
262.017555	8000.322813	13.865459	-0.054794	4.815552
262.077650	8000.304598	13.870464	-0.054805	4.815547
261.754953	8000.296107	13.875469	-0.054746	4.815546
262.122581	8000.348133	13.880474	-0.054814	4.815559
261.955763	8000.280237	13.885479	-0.054784	4.815540
262.018818	8000.254591	13.890483	-0.054796	4.815532
261.828464	8000.279265	13.895488	-0.054760	4.815541
261.892141	8000.255766	13.900493	-0.054773	4.815533
262.093441	8000.321080	13.905498	-0.054810	4.815552
262.200092	8000.265166	13.910503	-0.054831	4.815535
262.050979	8000.273424	13.915507	-0.054803	4.815538
261.926391	8000.295975	13.920512	-0.054780	4.815545
262.128922	8000.241640	13.925517	-0.054818	4.815528
262.195997	8000.302607	13.930522	-0.054831	4.815546
262.058448	8000.255494	13.935527	-0.054806	4.815532
262.101500	8000.241272	13.940531	-0.054814	4.815528
261.993603	8000.307906	13.945536	-0.054794	4.815548
261.985732	8000.284298	13.950541	-0.054793	4.815541
262.217638	8000.325541	13.955546	-0.054837	4.815552
261.967308	8000.247722	13.960551	-0.054790	4.815531
261.942159	8000.220624	13.965555	-0.054786	4.815523
262.179835	8000.297222	13.970560	-0.054831	4.815544
262.113201	8000.221359	13.975565	-0.054818	4.815522
261.963808	8000.317227	13.980570	-0.054791	4.815551
262.038727	8000.262927	13.985575	-0.054805	4.815535
262.147021	8000.254053	13.990579	-0.054826	4.815532
262.059946	8000.292181	13.995584	-0.054810	4.815543
262.074926	8000.244374	14.000589	-0.054813	4.815529
262.215379	8000.269153	14.005594	-0.054839	4.815536
262.046993	8000.297394	14.010599	-0.054808	4.815545
261.957264	8000.232904	14.015603	-0.054792	4.815526
262.031446	8000.246975	14.020608	-0.054806	4.815530
262.105310	8000.239671	14.025613	-0.054820	4.815528
262.157325	8000.314281	14.030618	-0.054830	4.815549
262.134882	8000.300049	14.035623	-0.054826	4.815545
262.177560	8000.302917	14.040627	-0.054835	4.815546
262.152897	8000.323908	14.045632	-0.054830	4.815552
262.058420	8000.298873	14.050637	-0.054813	4.815545
262.183978	8000.305243	14.055642	-0.054837	4.815546
261.895891	8000.288774	14.060647	-0.054783	4.815543
261.795123	8000.302101	14.065651	-0.054765	4.815547
262.111887	8000.275290	14.070656	-0.054824	4.815538
262.064133	8000.246751	14.075661	-0.054816	4.815530
261.917308	8000.282827	14.080666	-0.054789	4.815541
261.919171	8000.285022	14.085671	-0.054789	4.815542
262.064720	8000.313090	14.090675	-0.054817	4.815549
262.086291	8000.320953	14.095680	-0.054821	4.815551
261.909867	8000.288158	14.100685	-0.054789	4.815542
262.000380	8000.344169	14.105690	-0.054806	4.815558
261.927946	8000.323771	14.110695	-0.054793	4.815553
261.993221	8000.292820	14.115699	-0.054805	4.815543
262.077144	8000.285682	14.120704	-0.054821	4.815541
262.095070	8000.302032	14.125709	-0.054825	4.815546
262.106652	8000.341784	14.130714	-0.054827	4.815557
262.103471	8000.303294	14.135719	-0.054827	4.815546
262.107512	8000.274540	14.140723	-0.054828	4.815537
262.056088	8000.329282	14.145728	-0.054819	4.815554
262.124237	8000.315473	14.150733	-0.054832	4.815549
262.425646	8000.334355	14.155738	-0.054888	4.815553
262.155968	8000.275449	14.160743	-0.054838	4.815537
262.086655	8000.336308	14.165747	-0.054826	4.815556
262.238054	8000.339897	14.170752	-0.054854	4.815556
262.131645	8000.295433	14.175757	-0.054835	4.815543
261.966291	8000.318382	14.180762	-0.054804	4.815551
261.976796	8000.284391	14.185767	-0.054806	4.815541
262.155682	8000.323693	14.190771	-0.054840	4.815552
262.277235	8000.328929	14.195776	-0.054863	4.815552
262.067035	8000.282755	14.200781	-0.054824	4.815540
262.028395	8000.315270	14.205786	-0.054817	4.815550
261.999949	8000.279569	14.210791	-0.054812	4.815539
262.198782	8000.315995	14.215795	-0.054850	4.815549
262.145771	8000.337588	14.220800	-0.054840	4.815556
262.069459	8000.294688	14.225805	-0.054826	4.815543
261.994530	7999.295550	14.230810	-0.054812	4.815252

262.067724	7996.058723	14.235815	-0.054824	4.814306
262.090892	7990.595082	14.240819	-0.054825	4.812708
262.090021	7983.938378	14.245824	-0.054821	4.810762
261.907972	7976.612507	14.250829	-0.054782	4.808619
262.170631	7968.989821	14.255834	-0.054826	4.806387
261.919195	7961.173935	14.260839	-0.054775	4.804100
261.840226	7953.379433	14.265843	-0.054755	4.801817
261.799926	7945.337942	14.270848	-0.054743	4.799460
261.846570	7937.448609	14.275853	-0.054747	4.797146
261.828061	7929.408914	14.280858	-0.054738	4.794787
261.654725	7921.390077	14.285863	-0.054701	4.792434
261.690808	7913.336810	14.290867	-0.054703	4.790069
261.996890	7905.418816	14.295872	-0.054755	4.787741
261.580178	7897.368112	14.300877	-0.054673	4.785376
261.492783	7889.458748	14.305882	-0.054652	4.783051
261.786294	7881.412069	14.310887	-0.054701	4.780682
261.591775	7873.427409	14.315891	-0.054660	4.778332
261.508642	7865.415380	14.320896	-0.054640	4.775972
261.583076	7857.325728	14.325901	-0.054649	4.773588
261.545124	7849.421798	14.330906	-0.054637	4.771258
261.454574	7841.343327	14.335911	-0.054615	4.768875
261.554427	7833.371771	14.340915	-0.054629	4.766522
261.547096	7825.319305	14.345920	-0.054622	4.764144
261.364480	7817.414557	14.350925	-0.054584	4.761809
261.412298	7809.391886	14.355930	-0.054588	4.759438
261.327727	7801.371661	14.360935	-0.054567	4.757066
261.201381	7793.392975	14.365939	-0.054538	4.754706
261.119924	7785.351331	14.370944	-0.054518	4.752326
261.010519	7777.300799	14.375949	-0.054493	4.749942
260.973134	7769.332035	14.380954	-0.054481	4.747581
261.013331	7761.278598	14.385959	-0.054484	4.745193
260.971261	7753.346200	14.390963	-0.054471	4.742840
260.817784	7745.334577	14.395968	-0.054438	4.740463
260.756823	7737.327975	14.400973	-0.054421	4.738086
260.852458	7729.363747	14.405978	-0.054434	4.735720
260.740750	7721.312194	14.410983	-0.054409	4.733327
260.674501	7713.296684	14.415987	-0.054391	4.730944
260.863702	7705.299169	14.420992	-0.054422	4.728564
260.582903	7697.264624	14.425997	-0.054364	4.726173
260.686108	7689.345641	14.431002	-0.054379	4.723815
260.475461	7681.335655	14.436007	-0.054335	4.721428
260.431739	7673.291450	14.441011	-0.054322	4.719030
260.385204	7665.362257	14.446016	-0.054308	4.716666
260.358826	7657.287666	14.451021	-0.054298	4.714256
260.325006	7649.325881	14.456026	-0.054287	4.711879
260.322065	7641.247173	14.461031	-0.054282	4.709466
260.061221	7633.282402	14.466035	-0.054228	4.707086
260.117688	7625.295928	14.471040	-0.054234	4.704697
260.134909	7617.317386	14.476045	-0.054232	4.702310
260.256837	7609.273768	14.481050	-0.054250	4.699902
259.985259	7601.344111	14.486055	-0.054194	4.697528
260.138872	7593.259931	14.491059	-0.054218	4.695105
260.053042	7585.307434	14.496064	-0.054197	4.692721
259.998454	7577.231222	14.501069	-0.054182	4.690299
259.954280	7569.286158	14.506074	-0.054169	4.687915
259.894878	7561.268149	14.511079	-0.054153	4.685507
259.886916	7553.276400	14.516083	-0.054147	4.683107
259.764145	7545.331749	14.521088	-0.054119	4.680719
259.758411	7537.272463	14.526093	-0.054113	4.678295
260.017026	7529.300654	14.531098	-0.054156	4.675896
259.588269	7521.255883	14.536103	-0.054071	4.673475
259.684269	7513.142258	14.541107	-0.054084	4.671031
259.703843	7505.195120	14.546112	-0.054083	4.668636
259.524715	7497.169427	14.551117	-0.054045	4.666217
259.543889	7489.201552	14.556122	-0.054044	4.663813
259.626685	7481.245273	14.561127	-0.054054	4.661412
259.608982	7473.222413	14.566131	-0.054046	4.658989
259.419481	7465.308509	14.571136	-0.054006	4.656598
259.396575	7457.162856	14.576141	-0.053997	4.654136
259.745291	7449.227022	14.581146	-0.054057	4.651735
259.498330	7441.195425	14.586151	-0.054006	4.649305
259.408430	7433.253094	14.591155	-0.053984	4.646901
259.639664	7425.207546	14.596160	-0.054022	4.644463
259.342219	7417.235954	14.601165	-0.053962	4.642047
259.187674	7409.222626	14.606170	-0.053928	4.639618
259.106199	7401.238396	14.611175	-0.053908	4.637195
259.151632	7393.201023	14.616179	-0.053912	4.634755
259.333196	7385.177335	14.621184	-0.053941	4.632318
259.137338	7377.163450	14.626189	-0.053899	4.629883
259.139367	7369.206454	14.631194	-0.053895	4.627464
258.920293	7361.164142	14.636199	-0.053849	4.625018
258.833215	7353.193966	14.641203	-0.053828	4.622592
258.917977	7345.207619	14.646208	-0.053839	4.620160
258.886228	7337.185453	14.651213	-0.053828	4.617716
258.927903	7329.196239	14.656218	-0.053831	4.615280
259.034685	7321.183606	14.661223	-0.053846	4.612836
258.962951	7313.133282	14.666227	-0.053828	4.610379
258.848010	7305.204857	14.671232	-0.053801	4.607959
258.697910	7297.141720	14.676237	-0.053768	4.605495
258.956088	7289.167412	14.681242	-0.053812	4.603058
258.650626	7281.150819	14.686247	-0.053750	4.600606
258.499112	7273.177213	14.691251	-0.053717	4.598166
258.576622	7265.189249	14.696256	-0.053726	4.595721
258.617838	7257.106731	14.701261	-0.053729	4.593245
258.516019	7249.104171	14.706266	-0.053705	4.590793
258.207496	7241.116510	14.711271	-0.053643	4.588343
258.334800	7233.116045	14.716275	-0.053662	4.585889
258.501695	7225.144134	14.721280	-0.053688	4.583442
258.298462	7217.141778	14.726285	-0.053645	4.580984
258.320280	7209.114761	14.731290	-0.053644	4.578517
258.203183	7201.158452	14.736295	-0.053618	4.576071
258.097827	7193.095826	14.741299	-0.053593	4.573590
258.096893	7185.102178	14.746304	-0.053588	4.571130
258.172168	7177.056838	14.751309	-0.053597	4.568652
258.055071	7169.145186	14.756314	-0.053570	4.566214
258.131414	7161.101408	14.761319	-0.053580	4.563734
258.086926	7153.141391	14.766323	-0.053567	4.561279
257.987747	7145.177827	14.771328	-0.053543	4.558821
257.809494	7137.164375	14.776333	-0.053505	4.556346
258.022644	7129.113137	14.781338	-0.053540	4.553859
257.775816	7121.088632	14.786343	-0.053489	4.551378
257.660653	7113.058865	14.791347	-0.053463	4.548894
257.567447	7105.103009	14.796352	-0.053440	4.546431
257.702314	7097.052503	14.801357	-0.053461	4.543939
257.686920	7089.163359	14.806362	-0.053453	4.541495
257.491424	7081.128488	14.811367	-0.053412	4.539004
257.900120	7073.136763	14.816371	-0.053483	4.536526
257.655861	7065.119089	14.821376	-0.053432	4.534037
257.340264	7057.064156	14.826381	-0.053369	4.531535
257.499849	7049.085027	14.831386	-0.053394	4.529057
257.283925	7041.100699	14.836391	-0.053348	4.526575
257.294460	7033.071099	14.841395	-0.053345	4.524077
257.516558	7025.165787	14.846400	-0.053382	4.521618
257.346563	7017.083125	14.851405	-0.053345	4.519101
257.532762	7009.149633	14.856410	-0.053375	4.516630
257.487757	7001.052980	14.861415	-0.053362	4.514106
257.170841	6992.993056	14.866419	-0.053298	4.511591
257.148818	6985.051389	14.871424	-0.053289	4.509113
256.887164	6977.026127	14.876429	-0.053235	4.506607
257.131226	6969.043101	14.881434	-0.053276	4.504114
257.158913	6961.083265	14.886439	-0.053276	4.501626
257.008591	6953.068530	14.891443	-0.053243	4.499119
256.838384	6945.136310	14.896448	-0.053207	4.496636
256.833083	6937.065459	14.901453	-0.053201	4.494109
256.874160	6929.052518	14.906458	-0.053203	4.491599
256.825290	6921.012058	14.911463	-0.053189	4.489079
256.786966	6913.034753	14.916467	-0.053177	4.486577
256.887269	6905.046601	14.921472	-0.053191	4.484070
256.755756	6897.077188	14.926477	-0.053162	4.481568
256.684470	6889.078871	14.931482	-0.053144	4.479055
256.632536	6881.112675	14.936487	-0.053129	4.476551
256.651459	6873.022179	14.941491	-0.053128	4.474006
256.675589	6865.015574	14.946496	-0.053127	4.471487
256.611908	6856.977788	14.951501	-0.053111	4.468956
256.595602	6849.056988	14.956506	-0.053103	4.466460
256.558873	6841.013136	14.961511	-0.053091	4.463925
256.560261	6833.044678	14.966515	-0.053086	4.461412
256.528934	6825.044514	14.971520	-0.053076	4.458887
256.556462	6817.025450	14.976525	-0.053076	4.456355
256.655736	6809.031787	14.981530	-0.053089	4.453830
256.545408	6800.997867	14.986535	-0.053064	4.451290
256.424679	6793.001280	14.991539	-0.053036	4.448760
256.191690	6785.004834	14.996544	-0.052988	4.446228
256.135054	6777.004809	15.001549	-0.052973	4.443695
256.230287	6769.065470	15.006554	-0.052986	4.441180
256.134195	6761.043597	15.011559	-0.052963	4.438636
256.020213	6753.035468	15.016563	-0.052937	4.436096
255.945972	6744.983241	15.021568	-0.052918	4.433540
255.835276	6736.979453	15.026573	-0.052892	4.430997
255.844188	6728.956988	15.031578	-0.052889	4.428448
255.910419	6720.943224	15.036583	-0.052897	4.425901
255.662290	6712.930828	15.041587	-0.052846	4.423351
255.775094	6704.986419	15.046592	-0.052862	4.420822
255.801906	6696.977257	15.051597	-0.052862	4.418272
255.755554	6689.003217	15.056602	-0.052848	4.415730
255.743359	6680.955936	15.061607	-0.052841	4.413164
255.676301	6672.962143	15.066611	-0.052824	4.410614
255.763077	6664.976434	15.071616	-0.052835	4.408065
255.696152	6656.959676	15.076621	-0.052818	4.405504
255.493262	6649.016230	15.081626	-0.052775	4.402964
255.666288	6640.984410	15.086631	-0.052802	4.400397
255.564836	6632.989095	15.091635	-0.052778	4.397838
255.428664	6624.996140	15.096640	-0.052748	4.395278
255.397383	6616.960326	15.101645	-0.052737	4.392704
255.567384	6608.961805	15.106650	-0.052764	4.390141
255.221730	6600.983684	15.111655	-0.052695	4.387580
255.113073	6592.966318	15.116659	-0.052670	4.385007
255.349656	6584.994220	15.121664	-0.052709	4.382448
255.085900	6576.970607	15.126669	-0.052655	4.379869
255.008714	6569.026109	15.131674	-0.052636	4.377314
255.054961	6560.995722	15.136679	-0.052639	4.374732
255.035807	6552.960614	15.141683	-0.052631	4.372145
254.880531	6544.976441	15.146688	-0.052597	4.369573
254.903519	6537.004313	15.151693	-0.052597	4.367004
254.946401	6528.947438	15.156698	-0.052600	4.364407
254.773423	6521.035931	15.161703	-0.052563	4.361853
254.944649	6512.979314	15.166707	-0.052589	4.359254
255.071573	6505.050067	15.171712	-0.052608	4.356693
254.898340	6496.964353	15.176717	-0.052571	4.354079
254.832737	6488.884302	15.181722	-0.052554	4.351466
254.731165	6480.886068	15.186727	-0.052530	4.348877
254.593472	6472.893385	15.191731	-0.052500	4.346288
254.546132	6464.947008	15.196736	-0.052486	4.343713
254.390879	6456.948892	15.201741	-0.052452	4.341119
254.460134	6449.006700	15.206746	-0.052460	4.338544
254.504199	6440.978383	15.211751	-0.052463	4.335939
254.115235	6432.964182	15.216755	-0.052386	4.333333
254.314894	6424.957574	15.221760	-0.052418	4.330733
254.210552	6416.949872	15.226765	-0.052394	4.328129
254.317687	6408.926065	15.231770	-0.052409	4.325519
254.285931	6400.965762	15.236775	-0.052398	4.322927
254.206453	6392.920298	15.241779	-0.052378	4.320306
254.355617	6385.006728	15.246784	-0.052401	4.317728
253.996595	6376.933344	15.251789	-0.052330	4.315092
254.151981	6368.896237	15.256794	-0.052354	4.312471
253.960604	6360.912161	15.261799	-0.052313	4.309862
254.089078	6352.929334	15.266803	-0.052332	4.307255
254.204906	6344.906724	15.271808	-0.052349	4.304633
253.862352	6336.956166	15.276813	-0.052280	4.302030
253.779660	6328.923280	15.281818	-0.052260	4.299400
253.875960	6320.971066	15.286823	-0.052273	4.296796
253.762187	6312.918291	15.291827	-0.052247	4.294156
253.537610	6304.936061	15.296832	-0.052200	4.291537
253.465680	6296.889389	15.301837	-0.052182	4.288896
253.495941	6288.920255	15.306842	-0.052182	4.286280
253.576132	6280.914825	15.311847	-0.052193	4.283650
253.499104	6272.940108	15.316851	-0.052173	4.281028
253.581920	6264.963385	15.321856	-0.052184	4.278405
253.552968	6256.943199	15.326861	-0.052174	4.275765
253.482080	6248.853260	15.331866	-0.052155	4.273100
253.365389	6240.870937	15.336871	-0.052129	4.270469
253.211999	6232.879410	15.341875	-0.052095	4.267832
253.183812	6224.887679	15.346880	-0.052085	4.265195
253.309773	6216.881668	15.351885	-0.052104	4.262553
253.109969	6208.895009	15.356890	-0.052062	4.259912
253.009799	6200.907857	15.361895	-0.052038	4.257271
252.999551	6192.865700	15.366899	-0.052031	4.254611
253.106228	6184.890433	15.371904	-0.052046	4.251972
252.933823	6176.875034	15.376909	-0.052009	4.249316
252.812691	6168.941461	15.381914	-0.051982	4.246686
252.775952	6160.900372	15.386919	-0.051970	4.244019
252.824073	6152.933447	15.391923	-0.051974	4.241376
252.893297	6144.947374	15.396928	-0.051982	4.238725
252.505577	6136.922062	15.401933	-0.051905	4.236055
252.540227	6128.926407	15.406938	-0.051907	4.233397
252.622635	6120.871519	15.411943	-0.051917	4.230719
252.609813	6112.898562	15.416947	-0.051910	4.228065
252.640169	6104.909675	15.421952	-0.051910	4.225404
252.590890	6096.903825	15.426957	-0.051896	4.222735
252.578978	6088.962780	15.431962	-0.051889	4.220087
252.604503	6080.969493	15.436967	-0.051889	4.217420
252.607634	6072.907162	15.441971	-0.051885	4.214728
252.324048	6064.950239	15.446976	-0.051827	4.212066
252.280283	6056.880984	15.451981	-0.051814	4.209368
252.495816	6048.934886	15.456986	-0.051849	4.206712
252.237349	6040.912380	15.461991	-0.051796	4.204023
252.225188	6032.982474	15.466995	-0.051789	4.201367
252.041157	6024.942873	15.472000	-0.051750	4.198670
252.115263	6016.932013	15.477005	-0.051759	4.195984
252.206197	6008.873651	15.482010	-0.051771	4.193280
252.025212	6000.794758	15.487015	-0.051732	4.190565
252.242122	5992.867202	15.492019	-0.051768	4.187903
252.250266	5984.884530	15.497024	-0.051764	4.185219
251.784270	5976.917763	15.502029	-0.051673	4.182533
251.822195	5968.914800	15.507034	-0.051675	4.179839
251.862789	5960.904860	15.512039	-0.051678	4.177140
251.968061	5952.904425	15.517043	-0.051692	4.174444
251.618527	5944.919638	15.522048	-0.051622	4.171746
251.791028	5936.865367	15.527053	-0.051649	4.169029
251.565453	5928.906373	15.532058	-0.051603	4.166338
251.511467	5920.905260	15.537063	-0.051588	4.163633
251.407596	5912.920303	15.542067	-0.051563	4.160931
251.533568	5904.918876	15.547072	-0.051582	4.158224
251.298437	5896.905568	15.552077	-0.051533	4.155507
251.309051	5888.890931	15.557082	-0.051530	4.152791
251.267727	5880.850221	15.562087	-0.051518	4.150064
251.407611	5872.878366	15.567091	-0.051539	4.147360
251.529156	5864.869109	15.572096	-0.051557	4.144642
251.581916	5856.901483	15.577101	-0.051562	4.141935
251.415958	5848.915633	15.582106	-0.051526	4.139218
251.188498	5840.933635	15.587111	-0.051479	4.136499
251.151749	5832.873121	15.592115	-0.051467	4.133754
251.128076	5824.871555	15.597120	-0.051457	4.131028
250.915214	5816.858373	15.602125	-0.051413	4.128293
251.076100	5808.881747	15.607130	-0.051438	4.125574
251.096733	5800.923707	15.612135	-0.051437	4.122857
250.944827	5792.905113	15.617139	-0.051404	4.120116
250.816154	5784.947668	15.622144	-0.051375	4.117395
250.812008	5776.868632	15.627149	-0.051369	4.114631
250.969425	5768.842760	15.632154	-0.051394	4.111886
250.656715	5760.860892	15.637159	-0.051330	4.109148
250.562343	5752.871644	15.642163	-0.051308	4.106408
250.655642	5744.886075	15.647168	-0.051321	4.103671
250.575813	5736.880613	15.652173	-0.051301	4.100922
250.788248	5728.936545	15.657178	-0.051335	4.098196
250.694484	5720.923264	15.662183	-0.051313	4.095441
250.352327	5712.904211	15.667187	-0.051244	4.092679
250.385297	5704.916864	15.672192	-0.051246	4.089931
250.522064	5696.899987	15.677197	-0.051266	4.087172
250.618887	5688.910881	15.682202	-0.051279	4.084420
250.376845	5680.955956	15.687207	-0.051229	4.081674
250.195333	5672.945291	15.692211	-0.051191	4.078907
250.267494	5664.973363	15.697216	-0.051199	4.076155
250.171365	5656.909701	15.702221	-0.051176	4.073367
249.973232	5648.887324	15.707226	-0.051135	4.070591
250.195864	5640.903915	15.712231	-0.051171	4.067832
250.112064	5632.880667	15.717235	-0.051151	4.065052
250.118582	5624.951116	15.722240	-0.051147	4.062305
249.960294	5616.906810	15.727245	-0.051113	4.059514
250.077120	5608.980845	15.732250	-0.051130	4.056765
249.856313	5600.954707	15.737255	-0.051084	4.053975
249.943878	5592.945554	15.742259	-0.051095	4.051194
250.115581	5584.902431	15.747264	-0.051122	4.048400
249.793757	5576.890106	15.752269	-0.051057	4.045608
249.784455	5568.951778	15.757274	-0.051051	4.042844
249.756183	5560.931910	15.762279	-0.051040	4.040049
249.766658	5552.957129	15.767283	-0.051037	4.037269
249.718420	5544.930431	15.772288	-0.051024	4.034468
249.530202	5536.784865	15.777293	-0.050984	4.031622
249.506061	5528.849733	15.782298	-0.050974	4.028849
249.366486	5520.885830	15.787303	-0.050943	4.026063
249.229595	5512.881000	15.792307	-0.050913	4.023260
249.463064	5504.930613	15.797312	-0.050952	4.020480
249.398323	5496.940891	15.802317	-0.050935	4.017680
249.325505	5488.901049	15.807322	-0.050916	4.014860
249.369654	5480.931071	15.812327	-0.050919	4.012065
249.271674	5472.864540	15.817331	-0.050896	4.009231
249.228427	5464.938990	15.822336	-0.050883	4.006446
248.963108	5456.905602	15.827341	-0.050829	4.003618
249.065064	5448.909275	15.832346	-0.050843	4.000806
248.993597	5440.917557	15.837351	-0.050825	3.997991
248.845543	5432.898684	15.842355	-0.050792	3.995163
249.004236	5424.912203	15.847360	-0.050817	3.992350
248.978637	5416.869902	15.852365	-0.050807	3.989512
248.946511	5408.895516	15.857370	-0.050797	3.986696
248.814681	5400.881953	15.862375	-0.050767	3.983863
248.789896	5392.921236	15.867379	-0.050758	3.981048
248.887469	5384.934857	15.872384	-0.050771	3.978224
248.604414	5376.923539	15.877389	-0.050713	3.975382
248.789388	5368.928559	15.882394	-0.050743	3.972552
248.804100	5360.903271	15.887399	-0.050741	3.969707
248.668531	5352.925194	15.892403	-0.050711	3.966874
248.922753	5344.936003	15.897408	-0.050753	3.964041
248.859027	5336.978222	15.902413	-0.050736	3.961212
248.610639	5328.987668	15.907418	-0.050685	3.958367
248.486044	5320.995226	15.912423	-0.050657	3.955520
248.561137	5312.941932	15.917427	-0.050666	3.952654
248.461791	5304.959009	15.922432	-0.050643	3.949807
248.255594	5296.942493	15.927437	-0.050599	3.946944
248.417649	5288.946136	15.932442	-0.050625	3.944093
248.339781	5280.979574	15.937447	-0.050605	3.941247
247.899161	5273.007966	15.942451	-0.050518	3.938390
247.930348	5264.998798	15.947456	-0.050519	3.935526
247.976500	5256.958086	15.952461	-0.050523	3.932649
248.105355	5248.933910	15.957466	-0.050542	3.929777
248.119542	5240.998809	15.962471	-0.050540	3.926932
248.030338	5232.977240	15.967475	-0.050518	3.924053
248.004793	5225.016621	15.972480	-0.050509	3.921195
247.807094	5216.997614	15.977485	-0.050467	3.918311
247.791593	5209.026509	15.982490	-0.050459	3.915445
247.801365	5200.990562	15.987495	-0.050456	3.912554
247.739984	5192.961620	15.992499	-0.050440	3.909662
247.758484	5185.014208	15.997504	-0.050438	3.906799
247.604715	5176.966444	16.002509	-0.050405	3.903894
247.556548	5169.016972	16.007514	-0.050391	3.901024
247.680545	5161.010796	16.012519	-0.050409	3.898136
247.627623	5152.982655	16.017523	-0.050394	3.895233
247.638202	5144.985660	16.022528	-0.050391	3.892342
247.329835	5136.960587	16.027533	-0.050329	3.889431
247.404201	5129.040268	16.032538	-0.050338	3.886564
247.438091	5120.999633	16.037543	-0.050339	3.883650
247.286905	5112.977492	16.042547	-0.050306	3.880737
247.467208	5105.021905	16.047552	-0.050335	3.877853
247.356247	5097.019114	16.052557	-0.050309	3.874944
247.275825	5088.794117	16.057562	-0.050289	3.871952
247.084693	5080.844847	16.062567	-0.050249	3.869056
247.028217	5072.881436	16.067571	-0.050234	3.866155
247.096433	5064.929215	16.072576	-0.050241	3.863259
246.874733	5056.948322	16.077581	-0.050195	3.860344
246.918906	5048.994004	16.082586	-0.050199	3.857442
246.925763	5040.967392	16.087591	-0.050195	3.854511
246.870250	5032.975958	16.092595	-0.050180	3.851589
246.893006	5024.987977	16.097600	-0.050179	3.848668
246.797315	5017.008396	16.102605	-0.050156	3.845745
246.613478	5009.010895	16.107610	-0.050117	3.842812
246.692321	5001.031229	16.112615	-0.050127	3.839888
246.773963	4993.045548	16.117619	-0.050137	3.836960
246.809927	4985.033665	16.122624	-0.050139	3.834019
246.487069	4977.039777	16.127629	-0.050074	3.831075
246.424568	4969.031423	16.132634	-0.050058	3.828129
246.626851	4961.031108	16.137639	-0.050090	3.825189
246.678776	4953.025140	16.142643	-0.050095	3.822241
246.575888	4945.051165	16.147648	-0.050071	3.819300
246.481386	4937.083745	16.152653	-0.050049	3.816359
246.435874	4929.086707	16.157658	-0.050035	3.813406
246.354793	4921.065011	16.162663	-0.050015	3.810441
246.259025	4913.040328	16.167667	-0.049993	3.807471
246.147244	4905.099636	16.172672	-0.049967	3.804531
245.881092	4897.116885	16.177677	-0.049912	3.801569
245.923919	4889.105453	16.182682	-0.049915	3.798601
246.088804	4881.093907	16.187687	-0.049941	3.795633
245.845849	4873.047977	16.192691	-0.049891	3.792641
245.909670	4865.033964	16.197696	-0.049898	3.789666
245.811968	4857.067750	16.202701	-0.049875	3.786702
245.822315	4849.092133	16.207706	-0.049872	3.783735
245.689206	4841.114619	16.212711	-0.049842	3.780762
245.610089	4833.078221	16.217715	-0.049823	3.777765
245.734965	4825.090313	16.222720	-0.049841	3.774789
245.742776	4817.075614	16.227725	-0.049838	3.771798
245.580743	4809.098484	16.232730	-0.049803	3.768814
245.719862	4801.075994	16.237735	-0.049824	3.765818
245.564081	4793.123747	16.242739	-0.049790	3.762840
245.503563	4785.140354	16.247744	-0.049774	3.759849
245.344241	4777.129451	16.252749	-0.049739	3.756844
245.560575	4769.104337	16.257754	-0.049774	3.753839
245.526455	4761.078621	16.262759	-0.049763	3.750826
245.239068	4753.085080	16.267763	-0.049705	3.747817
245.350414	4745.108106	16.272768	-0.049720	3.744820
245.423279	4737.122460	16.277773	-0.049729	3.741818
245.137844	4729.125055	16.282778	-0.049671	3.738800
245.080566	4721.158809	16.287783	-0.049656	3.735796
245.017436	4713.135655	16.292787	-0.049639	3.732769
245.191855	4705.117237	16.297792	-0.049666	3.729746
245.144047	4697.140008	16.302797	-0.049653	3.726732
245.141703	4689.107760	16.307802	-0.049647	3.723695
245.034571	4681.186085	16.312807	-0.049623	3.720695
244.964648	4673.217374	16.317811	-0.049605	3.717676
245.139287	4665.180995	16.322816	-0.049632	3.714634
244.830132	4657.074528	16.327821	-0.049570	3.711552
244.769045	4649.103583	16.332826	-0.049553	3.708525
245.020589	4641.086053	16.337831	-0.049595	3.705485
244.788990	4633.149094	16.342835	-0.049547	3.702461
244.554828	4625.203312	16.347840	-0.049499	3.699431
244.408738	4617.244457	16.352845	-0.049467	3.696397
244.594764	4609.188549	16.357850	-0.049497	3.693330
244.747721	4601.171696	16.362855	-0.049520	3.690276
244.493502	4593.207908	16.367859	-0.049468	3.687229
244.512276	4585.219684	16.372864	-0.049467	3.684177
244.406720	4577.259385	16.377869	-0.049442	3.681130
244.540134	4569.242533	16.382874	-0.049462	3.678064
244.380774	4561.250229	16.387879	-0.049427	3.674999
244.412732	4553.207908	16.392883	-0.049428	3.671916
244.399275	4545.229055	16.397888	-0.049421	3.668854
244.472427	4537.243728	16.402893	-0.049430	3.665789
244.476802	4529.215302	16.407898	-0.049426	3.662703
244.324595	4521.230210	16.412903	-0.049392	3.659627
244.122200	4513.287733	16.417907	-0.049350	3.656564
244.267493	4505.267584	16.422912	-0.049372	3.653477
244.178830	4497.196505	16.427917	-0.049351	3.650362
244.117718	4489.240423	16.432922	-0.049334	3.647290
244.036380	4481.254501	16.437927	-0.049314	3.644202
243.940362	4473.278821	16.442931	-0.049292	3.641116
244.001671	4465.286180	16.447936	-0.049298	3.638024
243.818351	4457.290671	16.452941	-0.049259	3.634923
243.935495	4449.228872	16.457946	-0.049276	3.631801
243.751147	4441.287460	16.462951	-0.049237	3.628715
243.514883	4433.253654	16.467955	-0.049188	3.625589
243.787847	4425.291578	16.472960	-0.049234	3.622502
243.562077	4417.268522	16.477965	-0.049187	3.619375
243.519058	4409.330207	16.482970	-0.049174	3.616283
243.438796	4401.314042	16.487975	-0.049154	3.613157
243.423947	4393.269014	16.492979	-0.049146	3.610019
243.550086	4385.339302	16.497984	-0.049165	3.606927
243.390901	4377.312047	16.502989	-0.049130	3.603787
243.460515	4369.356932	16.507994	-0.049139	3.600678
243.530677	4361.379914	16.512999	-0.049147	3.597559
242.979630	4353.371535	16.518003	-0.049039	3.594406
243.142457	4345.371576	16.523008	-0.049065	3.591275
243.138467	4337.338080	16.528013	-0.049059	3.588122
243.038108	4329.344847	16.533018	-0.049035	3.584980
243.143169	4321.389810	16.538023	-0.049050	3.581857
243.064708	4313.367772	16.543027	-0.049031	3.578698
243.003155	4305.425325	16.548032	-0.049014	3.575569
243.039395	4297.379774	16.553037	-0.049016	3.572399
242.910657	4289.366111	16.558042	-0.048987	3.569235
242.875326	4281.431790	16.563047	-0.048976	3.566101
242.717373	4273.426637	16.568051	-0.048941	3.562933
242.712774	4265.447325	16.573056	-0.048936	3.559777
242.793224	4257.442779	16.578061	-0.048946	3.556611
242.949908	4249.393984	16.583066	-0.048970	3.553426
242.695167	4241.339713	16.588071	-0.048918	3.550225
242.492260	4233.401379	16.593075	-0.048875	3.547068
242.442550	4225.406108	16.598080	-0.048861	3.543890
242.443099	4217.407985	16.603085	-0.048856	3.540709
242.664257	4209.419262	16.608090	-0.048892	3.537537
242.626891	4201.422656	16.613095	-0.048880	3.534350
242.338499	4193.431928	16.618099	-0.048822	3.531155
242.361558	4185.469511	16.623104	-0.048821	3.527978
242.384456	4177.425994	16.628109	-0.048821	3.524766
242.450593	4169.491097	16.633114	-0.048828	3.521596
242.261671	4161.524329	16.638119	-0.048788	3.518402
242.116374	4153.510902	16.643123	-0.048756	3.515188
242.338577	4145.478199	16.648128	-0.048793	3.511974
242.247136	4137.474574	16.653133	-0.048771	3.508760
242.286707	4129.472876	16.658138	-0.048773	3.505547
242.204307	4121.513557	16.663143	-0.048753	3.502345
242.098100	4113.514548	16.668147	-0.048728	3.499123
241.956256	4105.585393	16.673152	-0.048697	3.495925
241.996232	4097.542557	16.678157	-0.048699	3.492684
241.995096	4089.524308	16.683162	-0.048694	3.489449
241.734869	4081.600254	16.688167	-0.048641	3.486240
241.499344	4073.602167	16.693171	-0.048592	3.483000
241.656564	4065.565281	16.698176	-0.048617	3.479753
241.459775	4057.637746	16.703181	-0.048575	3.476536
241.668026	4049.571658	16.708186	-0.048609	3.473273
241.643786	4041.537657	16.713191	-0.048600	3.470012
241.327738	4033.588983	16.718195	-0.048536	3.466774
241.430782	4025.603727	16.723200	-0.048550	3.463531
241.480035	4017.582658	16.728205	-0.048554	3.460269
241.638664	4009.607109	16.733210	-0.048579	3.457026
241.486153	4001.626453	16.738215	-0.048546	3.453767
241.473703	3993.614600	16.743219	-0.048539	3.450498
241.336609	3985.637980	16.748224	-0.048508	3.447235
241.265311	3977.643049	16.753229	-0.048490	3.443964
241.291926	3969.667639	16.758234	-0.048490	3.440701
241.042550	3961.712311	16.763239	-0.048439	3.437435
240.889939	3953.647949	16.768243	-0.048405	3.434123
241.060525	3945.647166	16.773248	-0.048432	3.430845
241.109625	3937.647187	16.778253	-0.048436	3.427561
241.120109	3929.647401	16.783258	-0.048434	3.424272
241.077184	3921.674855	16.788263	-0.048421	3.420989
240.921507	3913.707920	16.793267	-0.048387	3.417701
240.957708	3905.718495	16.798272	-0.048389	3.414408
240.770175	3897.713716	16.803277	-0.048349	3.411097
240.841016	3889.714989	16.808282	-0.048357	3.407795
240.837099	3881.735488	16.813287	-0.048351	3.404495
240.521635	3873.784436	16.818291	-0.048288	3.401192
240.562580	3865.824267	16.823296	-0.048291	3.397895
240.510402	3857.800620	16.828301	-0.048276	3.394565
240.642951	3849.664145	16.833306	-0.048296	3.391191
240.427257	3841.711427	16.838311	-0.048251	3.387879
240.314037	3833.732445	16.843315	-0.048225	3.384555
240.503426	3825.778480	16.848320	-0.048255	3.381250
240.272576	3817.837132	16.853325	-0.048207	3.377931
240.167692	3809.819710	16.858330	-0.048183	3.374582
240.220391	3801.809584	16.863335	-0.048188	3.371239
240.190625	3793.812182	16.868339	-0.048177	3.367894
240.041759	3785.845604	16.873344	-0.048145	3.364555
240.009640	3777.869553	16.878349	-0.048134	3.361212
240.010753	3769.874787	16.883354	-0.048129	3.357860
239.951219	3761.902150	16.888359	-0.048113	3.354511
239.731316	3753.871883	16.893363	-0.048067	3.351129
239.744876	3745.861540	16.898368	-0.048065	3.347761
239.927899	3737.840120	16.903373	-0.048094	3.344390
239.890212	3729.890302	16.908378	-0.048082	3.341038
239.872194	3721.949728	16.913383	-0.048074	3.337688
239.709288	3713.915253	16.918387	-0.048039	3.334289
239.688706	3705.943777	16.923392	-0.048030	3.330918
239.645571	3697.918942	16.928397	-0.048017	3.327521
239.616566	3689.943811	16.933402	-0.048007	3.324142
239.538988	3681.991386	16.938407	-0.047987	3.320767
239.279495	3673.992562	16.943411	-0.047934	3.317362
239.492086	3665.996319	16.948416	-0.047969	3.313972
239.478383	3657.930640	16.953421	-0.047961	3.310541
239.432905	3649.976558	16.958426	-0.047948	3.307153
239.260779	3642.016300	16.963431	-0.047911	3.303754
239.315853	3634.016263	16.968435	-0.047917	3.300343
239.222453	3626.063317	16.973440	-0.047894	3.296943
238.941500	3618.058061	16.978445	-0.047837	3.293509
239.043895	3610.033437	16.983450	-0.047851	3.290079
239.067253	3602.060664	16.988455	-0.047851	3.286664
238.966766	3594.059315	16.993459	-0.047827	3.283229
239.111339	3586.102395	16.998464	-0.047849	3.279818
238.949984	3578.126206	17.003469	-0.047814	3.276384
238.792029	3570.099406	17.008474	-0.047780	3.272924
238.899888	3562.078010	17.013479	-0.047795	3.269474
238.709714	3554.109562	17.018483	-0.047755	3.266031
238.885676	3546.137142	17.023488	-0.047783	3.262597
238.781307	3538.129356	17.028493	-0.047758	3.259133
238.802172	3530.157609	17.033498	-0.047757	3.255686
238.891350	3522.151986	17.038503	-0.047769	3.252224
238.473989	3514.182060	17.043507	-0.047686	3.248753
238.601600	3506.213711	17.048512	-0.047705	3.245300
238.573239	3498.204273	17.053517	-0.047695	3.241820
238.348470	3490.254662	17.058522	-0.047648	3.238354
238.506569	3482.250879	17.063527	-0.047673	3.234877
238.469794	3474.167789	17.068531	-0.047661	3.231353
238.656477	3466.193579	17.073536	-0.047691	3.227882
238.419959	3458.202385	17.078541	-0.047642	3.224383
238.182361	3450.265050	17.083546	-0.047593	3.220903
238.370983	3442.260771	17.088551	-0.047623	3.217407
238.012076	3434.281687	17.093555	-0.047551	3.213897
238.148560	3426.278340	17.098560	-0.047572	3.210392
238.086648	3418.288899	17.103565	-0.047556	3.206881
237.948656	3410.321825	17.108570	-0.047525	3.203373
237.834066	3402.352821	17.113575	-0.047499	3.199862
237.970397	3394.363123	17.118579	-0.047519	3.196348
238.057749	3386.362755	17.123584	-0.047531	3.192823
237.826108	3378.347896	17.128589	-0.047483	3.189274
237.781572	3370.348899	17.133594	-0.047469	3.185737
237.910755	3362.373201	17.138599	-0.047489	3.182213
237.611857	3354.397346	17.143603	-0.047428	3.178667
237.772612	3346.413079	17.148608	-0.047453	3.175133
237.803937	3338.394577	17.153613	-0.047454	3.171574
237.787203	3330.424097	17.158618	-0.047446	3.168031
237.460647	3322.446236	17.163623	-0.047380	3.164467
237.548978	3314.465331	17.168627	-0.047392	3.160915
237.856851	3306.476931	17.173632	-0.047444	3.157366
237.567856	3298.486260	17.178637	-0.047386	3.153785
237.350551	3290.492236	17.183642	-0.047340	3.150202
237.521252	3282.488335	17.188647	-0.047367	3.146628
237.329606	3274.498968	17.193651	-0.047327	3.143040
237.207124	3266.539168	17.198656	-0.047299	3.139465
237.127993	3258.573816	17.203661	-0.047279	3.135884
236.967226	3250.586774	17.208666	-0.047244	3.132287
236.895303	3242.598147	17.213671	-0.047226	3.128688
236.890368	3234.572658	17.218675	-0.047220	3.125071
237.027962	3226.633643	17.223680	-0.047241	3.121496
236.802250	3218.646447	17.228685	-0.047194	3.117878
236.695841	3210.667814	17.233690	-0.047170	3.114266
236.991886	3202.630830	17.238695	-0.047220	3.110641
236.947225	3194.630192	17.243699	-0.047206	3.107013
236.830218	3186.655786	17.248704	-0.047180	3.103389
236.648795	3178.679352	17.253709	-0.047141	3.099757
236.612483	3170.741009	17.258714	-0.047130	3.096145
236.408605	3162.750691	17.263719	-0.047087	3.092498
236.446979	3154.686634	17.268723	-0.047089	3.088823
236.736527	3146.724367	17.273728	-0.047138	3.085202
236.605561	3138.770832	17.278733	-0.047109	3.081561
236.364314	3130.790887	17.283738	-0.047059	3.077899
236.280206	3122.833212	17.288743	-0.047038	3.074250
236.284424	3114.707320	17.293747	-0.047034	3.070524
236.341493	3106.751024	17.298752	-0.047040	3.066873
236.172109	3098.778436	17.303757	-0.047003	3.063200
236.247418	3090.812829	17.308762	-0.047013	3.059538
236.017739	3082.896117	17.313767	-0.046965	3.055879
235.952707	3074.862540	17.318771	-0.046948	3.052169
236.096093	3066.878105	17.323776	-0.046970	3.048488
235.904147	3058.906784	17.328781	-0.046929	3.044792
235.714905	3050.949004	17.333786	-0.046889	3.041098
235.854130	3042.971036	17.338791	-0.046910	3.037406
235.762243	3034.952725	17.343795	-0.046888	3.033679
235.722654	3026.954993	17.348800	-0.046876	3.029960
235.667939	3018.952584	17.353805	-0.046861	3.026234
235.592962	3010.998335	17.358810	-0.046842	3.022524
235.448910	3003.041041	17.363815	-0.046810	3.018805
235.309562	2995.049714	17.368819	-0.046779	3.015066
235.571420	2987.026979	17.373824	-0.046823	3.011327
235.615150	2979.019658	17.378829	-0.046826	3.007580
235.510006	2971.053933	17.383834	-0.046802	3.003841
235.701325	2963.087536	17.388839	-0.046833	3.000111
235.631659	2955.120005	17.393843	-0.046815	2.996363
235.422668	2947.146060	17.398848	-0.046771	2.992600
235.350754	2939.117395	17.403853	-0.046753	2.988814
235.452423	2931.120853	17.408858	-0.046767	2.985047
235.288689	2923.202879	17.413863	-0.046731	2.981298
235.198188	2915.215238	17.418867	-0.046710	2.977516
235.260786	2907.228696	17.423872	-0.046717	2.973737
234.998023	2899.228512	17.428877	-0.046663	2.969931
234.859697	2891.259562	17.433882	-0.046632	2.966140
235.079948	2883.260409	17.438887	-0.046668	2.962349
234.958344	2875.297002	17.443891	-0.046641	2.958552
234.895517	2867.344095	17.448896	-0.046624	2.954759
234.792663	2859.315534	17.453901	-0.046600	2.950922
234.935784	2851.287197	17.458906	-0.046622	2.947093
234.835357	2843.351023	17.463911	-0.046598	2.943291
234.539213	2835.381923	17.468915	-0.046538	2.939458
234.833759	2827.413798	17.473920	-0.046588	2.935651
234.668855	2819.396113	17.478925	-0.046553	2.931791
234.433435	2811.412984	17.483930	-0.046504	2.927939
234.501255	2803.453989	17.488935	-0.046512	2.924110
234.599882	2795.465783	17.493939	-0.046525	2.920263
234.540614	2787.529271	17.498944	-0.046509	2.916427
234.395822	2779.461636	17.503949	-0.046477	2.912519
234.188067	2771.471120	17.508954	-0.046434	2.908639
234.121259	2763.510588	17.513959	-0.046416	2.904776
234.155297	2755.525121	17.518963	-0.046418	2.900901
234.077991	2747.577385	17.523968	-0.046399	2.897034
234.038639	2739.579694	17.528973	-0.046386	2.893139
234.051363	2731.568449	17.533978	-0.046384	2.889235
233.923546	2723.628400	17.538983	-0.046355	2.885353
233.759908	2715.675646	17.543987	-0.046320	2.881457
233.969394	2707.698471	17.548992	-0.046354	2.877565
233.720050	2699.726608	17.553997	-0.046303	2.873644
233.985658	2691.657870	17.559002	-0.046347	2.869699
233.783994	2683.731221	17.564007	-0.046305	2.865793
233.622437	2675.752653	17.569011	-0.046270	2.861858
233.753659	2667.785746	17.574016	-0.046289	2.857940
233.876901	2659.785703	17.579021	-0.046307	2.853999
233.622352	2651.788799	17.584026	-0.046255	2.850033
233.487664	2643.850761	17.589031	-0.046225	2.846098
233.508440	2635.859562	17.594035	-0.046224	2.842140
233.383949	2627.912322	17.599040	-0.046196	2.838189
233.268972	2619.934320	17.604045	-0.046170	2.834219
233.276914	2611.889605	17.609050	-0.046166	2.830217
233.276407	2603.931108	17.614055	-0.046161	2.826251
233.157522	2595.939164	17.619059	-0.046134	2.822256
233.173086	2588.000021	17.624064	-0.046132	2.818290
233.022808	2580.017494	17.629069	-0.046099	2.814287
232.947479	2572.021611	17.634074	-0.046081	2.810276
233.182687	2564.030670	17.639079	-0.046119	2.806280
233.133866	2556.043366	17.644083	-0.046105	2.802263
233.195582	2548.091973	17.649088	-0.046112	2.798265
232.987933	2540.138489	17.654093	-0.046069	2.794244
232.933587	2532.128122	17.659098	-0.046054	2.790198
233.086136	2524.145516	17.664103	-0.046077	2.786172
232.952844	2516.175534	17.669107	-0.046047	2.782130
232.812907	2508.232750	17.674112	-0.046016	2.778096
232.677532	2500.243897	17.679117	-0.045986	2.774032
232.724818	2492.223399	17.684122	-0.045990	2.769957
232.569588	2484.286159	17.689127	-0.045956	2.765907
232.403750	2476.318434	17.694131	-0.045921	2.761834
232.512820	2468.348000	17.699136	-0.045936	2.757770
232.361498	2460.357036	17.704141	-0.045903	2.753675
232.161848	2452.303944	17.709146	-0.045861	2.749538
232.273990	2444.354019	17.714151	-0.045877	2.745467
232.099857	2436.390738	17.719155	-0.045840	2.741366
232.275067	2428.430872	17.724160	-0.045867	2.737281
232.234466	2420.438134	17.729165	-0.045855	2.733160
232.236766	2412.433636	17.734170	-0.045851	2.729030
232.007767	2404.494714	17.739175	-0.045803	2.724913
232.235714	2396.527351	17.744179	-0.045841	2.720803
232.184597	2388.582320	17.749184	-0.045826	2.716681
231.938798	2380.600532	17.754189	-0.045776	2.712522
231.911466	2372.596575	17.759194	-0.045766	2.708359
231.981334	2364.636415	17.764199	-0.045774	2.704218
231.952638	2356.670335	17.769203	-0.045763	2.700061
232.041960	2348.698161	17.774208	-0.045775	2.695902
231.809165	2340.728741	17.779213	-0.045727	2.691718
231.693986	2332.748126	17.784218	-0.045701	2.687529
231.672855	2324.784105	17.789223	-0.045692	2.683348
231.603149	2316.805744	17.794227	-0.045674	2.679150
231.711566	2308.864549	17.799232	-0.045689	2.674976
231.369425	2300.870887	17.804237	-0.045621	2.670739
231.375751	2292.868987	17.809242	-0.045617	2.666514
231.705368	2284.873409	17.814247	-0.045673	2.662306
231.391782	2276.939900	17.819251	-0.045610	2.658082
231.282963	2268.991217	17.824256	-0.045585	2.653857
231.332597	2260.966015	17.829261	-0.045589	2.649595
231.213988	2253.029984	17.834266	-0.045562	2.645362
231.129613	2245.065952	17.839271	-0.045542	2.641110
231.016673	2237.112169	17.844275	-0.045516	2.636855
231.126069	2229.123494	17.849280	-0.045531	2.632589
230.863573	2221.144089	17.854285	-0.045478	2.628296
230.973082	2213.153125	17.859290	-0.045493	2.624015
230.859421	2205.210583	17.864295	-0.045467	2.619738
230.622988	2197.254866	17.869299	-0.045418	2.615438
230.710144	2189.258031	17.874304	-0.045430	2.611131
230.599978	2181.297421	17.879309	-0.045404	2.606823
230.791200	2173.306164	17.884314	-0.045435	2.602512
230.862221	2165.360861	17.889319	-0.045443	2.598210
230.667560	2157.371934	17.894323	-0.045402	2.593860
230.632051	2149.234080	17.899328	-0.045391	2.589432
230.576137	2141.289936	17.904333	-0.045375	2.585100
230.222163	2133.398534	17.909338	-0.045305	2.580770
230.373378	2125.445398	17.914343	-0.045328	2.576433
230.299533	2117.459536	17.919347	-0.045309	2.572055
230.201957	2109.524707	17.924352	-0.045286	2.567697
230.058052	2101.570361	17.929357	-0.045255	2.563317
230.006009	2093.620344	17.934362	-0.045240	2.558938
230.000524	2085.676932	17.939367	-0.045234	2.554559
229.926700	2077.669950	17.944371	-0.045215	2.550132
230.085257	2069.677560	17.949376	-0.045240	2.545722
230.009210	2061.736924	17.954381	-0.045221	2.541316
229.959432	2053.768821	17.959386	-0.045207	2.536889
229.986944	2045.821616	17.964391	-0.045207	2.532472
229.898409	2037.840929	17.969395	-0.045186	2.528020
229.720296	2029.907052	17.974400	-0.045148	2.523580
229.716571	2021.940060	17.979405	-0.045142	2.519126
229.711475	2013.975075	17.984410	-0.045136	2.514665
229.625551	2005.982349	17.989415	-0.045115	2.510175
229.443441	1998.007752	17.994419	-0.045077	2.505680
229.470914	1990.056555	17.999424	-0.045077	2.501205
229.617559	1982.076801	18.004429	-0.045099	2.496715
229.369920	1974.134143	18.009434	-0.045048	2.492209
229.317913	1966.166608	18.014439	-0.045034	2.487695
229.189481	1958.207798	18.019443	-0.045005	2.483172
229.254023	1950.257158	18.024448	-0.045012	2.478659
229.124269	1942.308963	18.029453	-0.044983	2.474126
229.099985	1934.302594	18.034458	-0.044974	2.469558
229.054895	1926.349793	18.039463	-0.044960	2.465011
228.867340	1918.411227	18.044467	-0.044921	2.460454
228.933291	1910.454849	18.049472	-0.044928	2.455896
228.892466	1902.466105	18.054477	-0.044916	2.451304
228.794835	1894.494657	18.059482	-0.044893	2.446709
228.920898	1886.541829	18.064487	-0.044911	2.442132
228.692664	1878.609157	18.069491	-0.044864	2.437532
228.598304	1870.623567	18.074496	-0.044841	2.432902
228.752900	1862.580293	18.079501	-0.044865	2.428250
228.752014	1854.625220	18.084506	-0.044860	2.423627
228.701025	1846.703467	18.089511	-0.044846	2.419012
228.372194	1838.776748	18.094515	-0.044780	2.414363
228.435546	1830.792072	18.099520	-0.044787	2.409702
228.380945	1822.839546	18.104525	-0.044772	2.405041
228.457675	1814.879655	18.109530	-0.044781	2.400377
228.429402	1806.949975	18.114535	-0.044771	2.395714
228.236623	1798.969807	18.119539	-0.044730	2.390999
228.287527	1791.000914	18.124544	-0.044735	2.386300
228.015854	1783.076111	18.129549	-0.044679	2.381593
228.236114	1775.082205	18.134554	-0.044715	2.376874
228.199358	1767.128299	18.139559	-0.044704	2.372150
227.960738	1759.183852	18.144563	-0.044654	2.367405
227.954526	1751.253470	18.149568	-0.044648	2.362678
227.955801	1743.302432	18.154573	-0.044644	2.357929
228.009730	1735.315205	18.159578	-0.044649	2.353154
227.904910	1727.346638	18.164583	-0.044625	2.348367
227.983281	1719.367222	18.169587	-0.044634	2.343579
227.791957	1711.465244	18.174592	-0.044594	2.338805
227.658398	1703.511444	18.179597	-0.044564	2.333996
227.687108	1695.528825	18.184602	-0.044565	2.329172
227.509088	1687.590879	18.189607	-0.044527	2.324348
227.151940	1679.685740	18.194611	-0.044455	2.319519
227.230769	1671.725159	18.199616	-0.044465	2.314683
227.420831	1663.698664	18.204621	-0.044495	2.309805
227.224130	1655.760862	18.209626	-0.044454	2.304939
227.191773	1647.838023	18.214631	-0.044443	2.300086
227.130419	1639.883543	18.219635	-0.044427	2.295201
226.907337	1631.945709	18.224640	-0.044380	2.290301
227.054275	1623.964651	18.229645	-0.044403	2.285396
226.982902	1616.028464	18.234650	-0.044385	2.280490
227.055125	1608.091315	18.239655	-0.044393	2.275584
226.649767	1600.097754	18.244659	-0.044313	2.270592
226.783785	1592.117799	18.249664	-0.044333	2.265644
226.873331	1584.164094	18.254669	-0.044345	2.260697
226.638560	1576.250303	18.259674	-0.044296	2.255737
226.661505	1568.298022	18.264679	-0.044296	2.250764
226.760237	1560.317167	18.269683	-0.044309	2.245768
226.671417	1552.410424	18.274688	-0.044288	2.240792
226.513618	1544.496269	18.279693	-0.044254	2.235793
226.553559	1536.508267	18.284698	-0.044256	2.230755
226.443485	1528.573825	18.289703	-0.044231	2.225725
226.025606	1520.662202	18.294707	-0.044148	2.220671
226.036291	1512.717004	18.299712	-0.044145	2.215622
226.271557	1504.717179	18.304717	-0.044184	2.210548
226.181263	1496.782621	18.309722	-0.044162	2.205474
225.957010	1488.887459	18.314727	-0.044116	2.200401
225.950373	1480.928861	18.319731	-0.044110	2.195296
226.031009	1472.953625	18.324736	-0.044120	2.190175
225.937486	1464.990902	18.329741	-0.044098	2.185036
225.840450	1457.059049	18.334746	-0.044075	2.179903
225.844629	1449.139019	18.339751	-0.044071	2.174776
225.643986	1441.189900	18.344755	-0.044028	2.169598
225.621281	1433.248684	18.349760	-0.044019	2.164430
225.594603	1425.327239	18.354765	-0.044010	2.159262
225.545956	1417.387589	18.359770	-0.043996	2.154067
225.437946	1409.447519	18.364775	-0.043971	2.148854
225.351182	1401.492403	18.369779	-0.043950	2.143621
225.352579	1393.566141	18.374784	-0.043945	2.138401
225.130367	1385.641943	18.379789	-0.043899	2.133150
225.339152	1377.655190	18.384794	-0.043933	2.127885
225.401823	1369.730212	18.389799	-0.043940	2.122634
225.344185	1361.806951	18.394803	-0.043924	2.117359
225.289222	1353.830575	18.399808	-0.043909	2.112036
225.135224	1345.878375	18.404813	-0.043875	2.106707
225.164270	1337.941776	18.409818	-0.043876	2.101392
224.926364	1330.055306	18.414823	-0.043827	2.096071
224.877717	1322.093271	18.419827	-0.043813	2.090704
225.065502	1314.140898	18.424832	-0.043843	2.085353
225.060362	1306.226012	18.429837	-0.043837	2.079995
224.684777	1298.363869	18.434842	-0.043762	2.074622
224.752502	1290.387135	18.439847	-0.043770	2.069201
224.547321	1282.454634	18.444851	-0.043727	2.063768
224.567703	1274.546174	18.449856	-0.043726	2.058361
224.501666	1266.612469	18.454861	-0.043709	2.052913
224.520337	1258.661135	18.459866	-0.043707	2.047447
224.588941	1250.732707	18.464871	-0.043715	2.041987
224.438457	1242.831682	18.469875	-0.043683	2.036509
224.424748	1234.880154	18.474880	-0.043675	2.030996
224.253960	1226.941734	18.479885	-0.043638	2.025460
224.256804	1219.021194	18.484890	-0.043634	2.019940
224.314126	1211.105083	18.489895	-0.043640	2.014413
224.194701	1203.155151	18.494899	-0.043613	2.008828
223.952774	1195.272156	18.499904	-0.043563	2.003263
223.844103	1187.371116	18.504909	-0.043538	1.997683
223.796511	1179.422045	18.509914	-0.043524	1.992060
223.920751	1171.473611	18.514919	-0.043542	1.986440
223.650832	1163.579046	18.519923	-0.043487	1.980800
223.750643	1155.649400	18.524928	-0.043501	1.975158
223.641355	1147.729690	18.529933	-0.043476	1.969485
223.600286	1139.803308	18.534938	-0.043463	1.963799
223.677519	1131.894539	18.539943	-0.043473	1.958121
223.379534	1123.972120	18.544947	-0.043413	1.952376
223.424392	1116.016612	18.549952	-0.043416	1.946627
223.463226	1108.098118	18.554957	-0.043419	1.940887
223.399086	1100.183983	18.559962	-0.043402	1.935123
223.334406	1092.281570	18.564967	-0.043385	1.929349
223.311799	1084.342180	18.569971	-0.043376	1.923536
223.372064	1076.445897	18.574976	-0.043382	1.917746
223.155807	1068.564387	18.579981	-0.043337	1.911919
222.995546	1060.634848	18.584986	-0.043302	1.906045
222.872503	1052.753034	18.589991	-0.043275	1.900191
222.836022	1044.840281	18.594995	-0.043263	1.894307
222.819729	1036.916011	18.600000	-0.043255	1.888398
222.622896	1029.031281	18.605005	-0.043214	1.882479
222.829866	1021.091468	18.610010	-0.043247	1.876546
222.826630	1013.179207	18.615015	-0.043242	1.870592
222.550001	1005.278128	18.620019	-0.043186	1.864595
222.559864	997.395893	18.625024	-0.043183	1.858626
222.436100	989.488018	18.630029	-0.043155	1.852603
222.346594	981.575327	18.635034	-0.043133	1.846560
222.331940	973.684419	18.640039	-0.043126	1.840524
222.086070	965.812668	18.645043	-0.043075	1.834454
222.155631	957.887635	18.650048	-0.043083	1.828361
222.173286	949.979564	18.655053	-0.043082	1.822254
222.165171	942.076586	18.660058	-0.043075	1.816128
222.060529	934.184490	18.665063	-0.043051	1.809978
221.885832	926.307538	18.670067	-0.043014	1.803810
221.997701	918.413269	18.675072	-0.043030	1.797642
221.971100	910.477377	18.680077	-0.043020	1.791403
221.499108	902.606819	18.685082	-0.042927	1.785140
221.584433	894.721378	18.690087	-0.042938	1.778911
221.474860	886.830960	18.695091	-0.042913	1.772632
221.412109	878.938967	18.700096	-0.042896	1.766336
221.396583	871.057431	18.705101	-0.042889	1.760031
221.363669	863.180996	18.710106	-0.042878	1.753705
221.483805	855.252545	18.715111	-0.042895	1.747334
221.259165	847.393332	18.720115	-0.042849	1.740952
221.274743	839.524871	18.725120	-0.042847	1.734569
221.320134	831.619214	18.730125	-0.042850	1.728136
221.156651	823.764279	18.735130	-0.042815	1.721694
221.161756	815.901693	18.740135	-0.042811	1.715243
221.031803	808.003072	18.745139	-0.042782	1.708721
220.908456	800.140612	18.750144	-0.042754	1.702204
220.736250	792.292950	18.755149	-0.042718	1.695668
220.771253	784.383628	18.760154	-0.042719	1.689083
220.743424	776.529343	18.765159	-0.042709	1.682510
220.578512	768.678650	18.770163	-0.042674	1.675895
220.753472	760.760232	18.775168	-0.042701	1.669243
220.721735	752.899530	18.780173	-0.042691	1.662585
220.442467	745.078670	18.785178	-0.042634	1.655901
220.267968	737.235138	18.790183	-0.042597	1.649184
220.272610	729.354935	18.795187	-0.042593	1.642433
220.430187	721.485187	18.800192	-0.042617	1.635684
220.199865	713.587598	18.805197	-0.042570	1.628830
219.957005	705.754159	18.810202	-0.042520	1.622000
220.166360	697.874137	18.815207	-0.042554	1.615164
220.057735	690.019778	18.820211	-0.042529	1.608277
219.783670	682.216982	18.825216	-0.042473	1.601382
219.738880	674.373210	18.830221	-0.042460	1.594454
219.726103	666.499483	18.835226	-0.042453	1.587473
219.744000	658.657133	18.840231	-0.042451	1.580494
219.508069	650.842546	18.845235	-0.042402	1.573473
219.662352	642.963418	18.850240	-0.042426	1.566418
219.597939	635.141948	18.855245	-0.042409	1.559351
219.380755	627.323263	18.860250	-0.042364	1.552233
219.346428	619.468896	18.865255	-0.042353	1.545076
219.302432	611.637463	18.870259	-0.042340	1.537905
219.242575	603.809513	18.875264	-0.042324	1.530701
219.214662	595.978963	18.880269	-0.042314	1.523466
219.003382	588.187215	18.885274	-0.042270	1.516205
218.999821	580.345138	18.890279	-0.042265	1.508893
219.047478	572.503371	18.895283	-0.042269	1.501553
218.960484	564.711373	18.900288	-0.042248	1.494204
218.849255	556.897166	18.905293	-0.042222	1.486794
218.796436	549.094044	18.910298	-0.042208	1.479366
218.800264	541.259365	18.915303	-0.042204	1.471879
218.684036	533.421417	18.920307	-0.042177	1.464332
218.413940	525.667581	18.925312	-0.042122	1.456803
218.584821	517.821830	18.930317	-0.042149	1.449215
218.373247	510.054149	18.935322	-0.042105	1.441603
218.361644	502.271976	18.940327	-0.042098	1.433968
218.343426	494.440835	18.945331	-0.042090	1.426243
218.460776	486.649719	18.950336	-0.042107	1.418537
218.128980	478.911584	18.955341	-0.042040	1.410769
218.160649	471.116260	18.960346	-0.042042	1.402960
218.261067	463.327598	18.965351	-0.042056	1.395126
218.107385	455.539241	18.970355	-0.042022	1.387205
217.891120	447.809658	18.975360	-0.041977	1.379288
217.827171	440.035211	18.980365	-0.041960	1.371305
217.847558	432.252400	18.985370	-0.041960	1.363281
217.716821	424.525446	18.990375	-0.041930	1.355241
217.707603	416.735369	18.995379	-0.041924	1.347109
217.820033	408.972533	19.000384	-0.041940	1.338977
217.455482	401.273691	19.005389	-0.041868	1.330779
217.463773	393.518761	19.010394	-0.041864	1.322537
217.414896	385.764718	19.015399	-0.041851	1.314234
217.322210	377.907304	19.020403	-0.041828	1.305758
217.076834	370.231144	19.025408	-0.041778	1.297396
216.937908	362.516130	19.030413	-0.041748	1.288957
217.226777	354.740279	19.035418	-0.041797	1.280474
217.179466	347.055150	19.040423	-0.041783	1.271973
216.848369	339.379219	19.045427	-0.041717	1.263371
216.964462	331.662731	19.050432	-0.041734	1.254750
216.854762	323.965744	19.055437	-0.041708	1.246048
216.869298	316.275301	19.060442	-0.041707	1.237315
216.793114	308.583466	19.065447	-0.041688	1.228502
216.506258	300.932088	19.070451	-0.041630	1.219630
216.463582	293.255134	19.075456	-0.041617	1.210712
216.587975	285.555166	19.080461	-0.041635	1.201734
216.385696	277.923794	19.085466	-0.041593	1.192703
216.238624	270.275477	19.090471	-0.041561	1.183595
216.193736	262.624278	19.095475	-0.041548	1.174433
216.095020	254.985004	19.100480	-0.041525	1.165203
216.011607	247.367616	19.105485	-0.041505	1.155929
215.971466	239.685000	19.110490	-0.041493	1.146509
216.090327	232.045810	19.115495	-0.041510	1.137098
215.726996	224.470007	19.120499	-0.041438	1.127584
215.587524	216.888567	19.125504	-0.041407	1.118031
215.680327	209.261839	19.130509	-0.041420	1.108388
215.569803	201.680379	19.135514	-0.041395	1.098675
215.588904	194.092853	19.140519	-0.041394	1.088895
215.383252	186.549452	19.145523	-0.041351	1.079034
215.399651	178.970586	19.150528	-0.041349	1.069085
215.118190	171.454549	19.155533	-0.041292	1.059059
214.986625	163.919062	19.160538	-0.041263	1.048945
214.856912	156.408528	19.165543	-0.041234	1.038766
214.678239	148.896781	19.170547	-0.041196	1.028474
214.673241	141.382957	19.175552	-0.041191	1.018116
214.745518	133.864747	19.180557	-0.041200	1.007665
214.817284	126.365011	19.185562	-0.041209	0.997130
214.511758	118.905824	19.190567	-0.041147	0.986447
214.370952	111.458355	19.195571	-0.041116	0.975704
214.449556	103.988522	19.200576	-0.041126	0.964866
214.371116	96.574543	19.205581	-0.041107	0.953946
213.944412	89.208154	19.210586	-0.041023	0.942880
213.868317	81.820035	19.215591	-0.041005	0.931743
213.786446	74.435690	19.220595	-0.040985	0.920474
213.839156	67.051238	19.225600	-0.040990	0.909103
213.370771	59.999043	19.230605	-0.040899	0.897966