Thu Mar 11 18:46:47 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.260165	0.097863	0.000000	0.000034	0.724885

0.476537	0.061156	0.005005	-0.000006	0.724889
0.236601	-0.045529	0.010010	0.000038	0.724597
0.206785	-0.040364	0.015014	0.000043	0.724597
0.330092	-0.065529	0.020019	0.000020	0.724592
0.352290	-0.069743	0.025024	0.000016	0.724591
0.209214	-0.041982	0.030029	0.000042	0.724596
0.346016	-0.071663	0.035034	0.000017	0.724586
0.397195	-0.073978	0.040038	0.000007	0.724600
0.193407	-0.042227	0.045043	0.000044	0.724592
0.148719	-0.034015	0.050048	0.000053	0.724593
0.367876	-0.073174	0.055053	0.000012	0.724593
0.311048	-0.066749	0.060058	0.000022	0.724586
0.204754	-0.043302	0.065062	0.000041	0.724595
0.431814	-0.087457	0.070067	-0.000001	0.724588
0.462297	-0.092628	0.075072	-0.000007	0.724589
0.427337	-0.103734	0.080077	-0.000001	0.724556
0.292147	-0.235096	0.085082	0.000024	0.724252
0.386287	-0.247614	0.090086	0.000007	0.724261
0.462386	-0.264494	0.095091	-0.000008	0.724255
0.238698	-0.224533	0.100096	0.000034	0.724255
0.418568	-0.253510	0.105101	-0.000000	0.724262
0.403706	-0.254355	0.110106	0.000002	0.724255
0.364231	-0.366035	0.115110	0.000010	0.724023
0.330003	-0.397140	0.120115	0.000016	0.723951
0.234952	-0.382552	0.125120	0.000033	0.723947
0.403121	-0.407615	0.130125	0.000002	0.723957
0.290058	-0.391811	0.135130	0.000022	0.723949
0.493949	-0.557524	0.140134	-0.000016	0.723696
0.401625	-0.575362	0.145139	0.000001	0.723629
0.235268	-0.547439	0.150144	0.000032	0.723626
0.394155	-0.573043	0.155149	0.000002	0.723632
0.248341	-0.650956	0.160154	0.000029	0.723428
0.243267	-0.693870	0.165158	0.000030	0.723343
0.250533	-0.698650	0.170163	0.000028	0.723337
0.319410	-0.709822	0.175168	0.000015	0.723339
0.316938	-0.863477	0.180173	0.000016	0.723037
0.244824	-0.869562	0.185178	0.000029	0.723001
0.307454	-0.878309	0.190182	0.000017	0.723006
0.278240	-0.967664	0.195187	0.000022	0.722821
0.105513	-1.004753	0.200192	0.000054	0.722688
0.241311	-1.025536	0.205197	0.000029	0.722695
0.137365	-1.078081	0.210202	0.000048	0.722556
0.175591	-1.178271	0.215206	0.000041	0.722373
-0.036448	-1.145907	0.220211	0.000080	0.722363
0.036411	-1.222508	0.225216	0.000066	0.722239
-0.128582	-1.274430	0.230221	0.000097	0.722080
-0.127282	-1.280448	0.235226	0.000096	0.722069
0.001664	-1.394146	0.240230	0.000072	0.721891
-0.004272	-1.469704	0.245235	0.000073	0.721741
-0.149660	-1.444713	0.250240	0.000100	0.721739
-0.099713	-1.587031	0.255245	0.000090	0.721478
-0.172786	-1.599812	0.260250	0.000104	0.721427
-0.262838	-1.626678	0.265254	0.000120	0.721343
-0.435962	-1.712412	0.270259	0.000152	0.721115
-0.287559	-1.737871	0.275264	0.000124	0.721117
-0.189469	-1.848615	0.280269	0.000106	0.720934
-0.524751	-1.821348	0.285274	0.000168	0.720871
-0.435265	-1.893242	0.290278	0.000151	0.720761
-0.411825	-2.008334	0.295283	0.000147	0.720543
-0.490005	-2.000027	0.300288	0.000161	0.720533
-0.503962	-2.152939	0.305293	0.000164	0.720227
-0.763156	-2.111958	0.310298	0.000212	0.720217
-0.902237	-2.203609	0.315302	0.000237	0.719988
-1.643742	-2.118849	0.320307	0.000375	0.719896
-2.056745	-2.080898	0.325312	0.000452	0.719826
-2.808385	-2.061410	0.330317	0.000591	0.719601
-2.826023	-2.063679	0.335322	0.000594	0.719591
-3.152012	-2.045483	0.340326	0.000655	0.719513
-4.230556	-1.979950	0.345331	0.000855	0.719264
-3.738834	-2.068657	0.350336	0.000764	0.719262
-4.051356	-2.011518	0.355341	0.000822	0.719265
-4.951660	-1.976731	0.360346	0.000989	0.719018
-5.168556	-1.967682	0.365350	0.001029	0.718960
-4.829130	-2.033459	0.370355	0.000966	0.718950
-5.258739	-1.956575	0.375360	0.001046	0.718951
-5.551159	-2.011877	0.380365	0.001100	0.718740
-6.367656	-1.920345	0.385370	0.001252	0.718634
-5.717979	-2.031493	0.390374	0.001130	0.718643
-6.162185	-1.955843	0.395379	0.001213	0.718637
-6.320685	-1.942191	0.400384	0.001242	0.718609
-6.518943	-2.035397	0.405389	0.001279	0.718355
-7.287727	-1.904781	0.410394	0.001422	0.718343
-7.211011	-1.912658	0.415398	0.001407	0.718355
-6.766162	-1.994879	0.420403	0.001324	0.718350
-7.147368	-1.937918	0.425408	0.001395	0.718329
-7.893612	-1.963062	0.430413	0.001534	0.718017
-7.840216	-1.975837	0.435418	0.001523	0.718011
-8.172194	-1.912584	0.440422	0.001585	0.718019
-8.341957	-1.885454	0.445427	0.001616	0.718014
-8.165730	-1.918803	0.450432	0.001583	0.718010
-7.774519	-2.026197	0.455437	0.001510	0.717936
-8.945169	-1.939168	0.460442	0.001728	0.717697
-8.857877	-1.951660	0.465446	0.001711	0.717703
-8.788869	-1.967334	0.470451	0.001698	0.717697
-9.199032	-1.895013	0.475456	0.001775	0.717696
-9.183267	-1.895279	0.480461	0.001771	0.717701
-9.054227	-1.935111	0.485466	0.001747	0.717668
-9.281232	-2.041176	0.490470	0.001789	0.717379
-10.046466	-1.906476	0.495475	0.001931	0.717376
-10.448161	-1.836886	0.500480	0.002006	0.717373
-9.498556	-2.002226	0.505485	0.001829	0.717381
-9.794122	-1.953907	0.510490	0.001884	0.717373
-9.911202	-1.930946	0.515494	0.001905	0.717378
-9.894438	-2.038899	0.520499	0.001902	0.717170
-11.097661	-1.870255	0.525504	0.002126	0.717080
-10.984128	-1.887031	0.530509	0.002104	0.717088
-10.917923	-1.904767	0.535514	0.002092	0.717076
-10.699527	-1.940695	0.540518	0.002051	0.717083
-10.894382	-1.908655	0.545523	0.002087	0.717078
-10.934474	-1.902013	0.550528	0.002094	0.717077
-10.823193	-2.059609	0.555533	0.002073	0.716805
-12.021076	-1.875324	0.560538	0.002296	0.716748
-11.874434	-1.896462	0.565542	0.002268	0.716758
-11.402074	-1.983822	0.570547	0.002180	0.716752
-11.590168	-1.951644	0.575552	0.002215	0.716750
-11.816832	-1.909086	0.580557	0.002257	0.716755
-11.967226	-1.888000	0.585562	0.002285	0.716744
-11.992576	-2.033531	0.590566	0.002289	0.716448
-12.556082	-1.935700	0.595571	0.002394	0.716443
-13.080101	-1.843485	0.600576	0.002491	0.716441
-12.374122	-1.967139	0.605581	0.002360	0.716446
-12.482805	-1.951549	0.610586	0.002380	0.716439
-12.753207	-1.899899	0.615590	0.002430	0.716446
-12.429234	-1.981797	0.620595	0.002369	0.716399
-13.248203	-1.972958	0.625600	0.002522	0.716128
-13.180016	-1.981624	0.630605	0.002509	0.716135
-13.789561	-1.878465	0.635610	0.002622	0.716125
-13.485765	-1.928589	0.640614	0.002565	0.716133
-13.721877	-1.888603	0.645619	0.002609	0.716129
-13.977601	-1.845281	0.650624	0.002656	0.716125
-13.186404	-1.988966	0.655629	0.002509	0.716120
-14.119641	-1.946401	0.660634	0.002682	0.715876
-14.501791	-1.876145	0.665638	0.002753	0.715881
-14.357134	-1.904381	0.670643	0.002726	0.715876
-14.044262	-1.960417	0.675648	0.002667	0.715876
-14.265483	-1.917923	0.680653	0.002708	0.715882
-14.704789	-1.844378	0.685658	0.002790	0.715874
-13.910844	-2.019273	0.690662	0.002642	0.715808
-15.031882	-1.954491	0.695667	0.002850	0.715541
-15.495531	-1.874047	0.700672	0.002936	0.715537
-15.381974	-1.889578	0.705677	0.002915	0.715547
-15.225368	-1.923328	0.710682	0.002886	0.715535
-15.194979	-1.925027	0.715686	0.002880	0.715543
-15.262715	-1.915939	0.720691	0.002892	0.715538
-15.330993	-1.911281	0.725696	0.002905	0.715523
-15.819782	-1.971228	0.730701	0.002995	0.715232
-16.385864	-1.875602	0.735706	0.003101	0.715222
-16.351589	-1.879295	0.740710	0.003094	0.715228
-15.966708	-1.948948	0.745715	0.003022	0.715226
-16.502420	-1.853263	0.750720	0.003122	0.715227
-16.061992	-1.928090	0.755725	0.003039	0.715234
-15.852306	-1.972750	0.760730	0.003000	0.715220
-16.930502	-1.930815	0.765734	0.003201	0.714923
-17.206140	-1.891961	0.770739	0.003252	0.714903
-17.123739	-1.908594	0.775744	0.003236	0.714900
-16.696065	-1.980720	0.780749	0.003156	0.714908
-17.252082	-1.885703	0.785754	0.003260	0.714901
-16.902584	-1.943547	0.790758	0.003194	0.714910
-16.518392	-2.015950	0.795763	0.003123	0.714902
-17.819324	-1.936344	0.800768	0.003365	0.714601
-17.943196	-1.910606	0.805773	0.003387	0.714608
-17.943126	-1.917013	0.810778	0.003387	0.714596
-17.725521	-1.950499	0.815782	0.003346	0.714607
-17.869385	-1.928512	0.820787	0.003373	0.714600
-18.149539	-1.879452	0.825792	0.003425	0.714599
-17.700179	-1.957490	0.830797	0.003341	0.714604
-18.519156	-1.968862	0.835802	0.003493	0.714292
-18.814825	-1.924738	0.840806	0.003548	0.714275
-18.935533	-1.905735	0.845811	0.003570	0.714271
-19.091600	-1.876974	0.850816	0.003599	0.714273
-18.917988	-1.905887	0.855821	0.003567	0.714277
-18.879426	-1.916830	0.860826	0.003559	0.714270
-19.009505	-1.890656	0.865830	0.003583	0.714276
-19.166741	-1.924746	0.870835	0.003612	0.714153
-19.824843	-1.902622	0.875840	0.003734	0.713965
-19.360669	-1.980987	0.880845	0.003648	0.713974
-20.249501	-1.828665	0.885850	0.003813	0.713962
-20.022496	-1.865208	0.890854	0.003771	0.713970
-19.636125	-1.935210	0.895859	0.003698	0.713968
-20.166147	-1.843751	0.900864	0.003797	0.713963
-20.011030	-1.866544	0.905869	0.003768	0.713973
-20.351269	-1.956344	0.910874	0.003831	0.713674
-20.699864	-1.904351	0.915878	0.003896	0.713655
-20.812880	-1.887893	0.920883	0.003916	0.713648
-20.776649	-1.895316	0.925888	0.003909	0.713646
-20.766162	-1.894777	0.930893	0.003907	0.713652
-21.046842	-1.849035	0.935898	0.003959	0.713644
-20.618388	-1.921511	0.940902	0.003879	0.713652
-20.562456	-2.017622	0.945907	0.003869	0.713481
-22.063828	-1.814627	0.950912	0.004148	0.713353
-21.511848	-1.908683	0.955917	0.004045	0.713362
-21.430522	-1.928771	0.960922	0.004029	0.713351
-21.661193	-1.883893	0.965926	0.004072	0.713359
-21.753990	-1.869426	0.970931	0.004089	0.713356
-21.834339	-1.856823	0.975936	0.004104	0.713353
-21.326045	-2.026630	0.980941	0.004009	0.713196
-22.891765	-1.838258	0.985946	0.004300	0.713016
-22.605647	-1.886047	0.990950	0.004247	0.713022
-22.380223	-1.929455	0.995955	0.004205	0.713016
-22.568697	-1.897939	1.000960	0.004240	0.713013
-22.250395	-1.950365	1.005965	0.004180	0.713022
-22.536734	-1.905570	1.010970	0.004233	0.713010
-22.506616	-1.978807	1.015974	0.004227	0.712875
-23.754849	-1.844289	1.020979	0.004459	0.712701
-23.746996	-1.846538	1.025984	0.004458	0.712699
-23.370167	-1.911003	1.030989	0.004387	0.712705
-23.738104	-1.849116	1.035994	0.004456	0.712698
-23.627180	-1.865575	1.040998	0.004435	0.712705
-23.615323	-1.869400	1.046003	0.004432	0.712702
-23.766527	-1.844249	1.051008	0.004460	0.712699
-23.797142	-1.918862	1.056013	0.004466	0.712540
-24.501994	-1.873397	1.061018	0.004597	0.712381
-24.236802	-1.918678	1.066022	0.004547	0.712386
-24.584203	-1.858685	1.071027	0.004612	0.712382
-24.631332	-1.851137	1.076032	0.004620	0.712381
-24.004796	-1.958726	1.081037	0.004503	0.712389
-24.632935	-1.852276	1.086042	0.004620	0.712379
-24.548758	-1.898960	1.091046	0.004604	0.712316
-25.204694	-1.896612	1.096051	0.004726	0.712089
-24.967972	-1.940112	1.101056	0.004682	0.712086
-25.507802	-1.840463	1.106061	0.004782	0.712094
-25.410418	-1.862620	1.111066	0.004764	0.712085
-25.016176	-1.932974	1.116070	0.004690	0.712085
-25.203029	-1.898727	1.121075	0.004724	0.712087
-25.486604	-1.885548	1.126080	0.004777	0.712013
-26.033856	-1.914689	1.131085	0.004879	0.711761
-26.325902	-1.865338	1.136090	0.004933	0.711756
-26.438692	-1.842252	1.141094	0.004954	0.711763
-26.098501	-1.905011	1.146099	0.004890	0.711759
-26.385585	-1.855096	1.151104	0.004943	0.711757
-26.538475	-1.824591	1.156109	0.004971	0.711764
-26.250902	-1.881067	1.161114	0.004918	0.711754
-26.427654	-1.951993	1.166118	0.004950	0.711550
-27.436227	-1.822545	1.171123	0.005138	0.711450
-27.230649	-1.861005	1.176128	0.005099	0.711447
-26.536149	-1.979779	1.181133	0.004970	0.711457
-26.935815	-1.915318	1.186138	0.005044	0.711444
-27.338581	-1.839192	1.191142	0.005119	0.711453
-26.831343	-1.930818	1.196147	0.005024	0.711451
-27.212237	-1.990200	1.201152	0.005095	0.711198
-28.258913	-1.834299	1.206157	0.005289	0.711137
-28.317832	-1.825586	1.211162	0.005300	0.711134
-27.845468	-1.907480	1.216166	0.005212	0.711139
-28.097285	-1.865293	1.221171	0.005259	0.711134
-28.294835	-1.831408	1.226176	0.005295	0.711132
-27.693815	-1.934820	1.231181	0.005183	0.711140
-27.981916	-1.956405	1.236186	0.005237	0.710995
-28.921036	-1.852344	1.241190	0.005411	0.710869
-28.480844	-1.931635	1.246195	0.005329	0.710868
-28.737263	-1.888236	1.251200	0.005376	0.710863
-28.867071	-1.858836	1.256205	0.005400	0.710876
-28.795303	-1.876305	1.261210	0.005387	0.710868
-28.505520	-1.926408	1.266214	0.005333	0.710871
-29.307681	-1.937650	1.271219	0.005482	0.710564
-30.128712	-1.811256	1.276224	0.005634	0.710524
-29.645933	-1.892784	1.281229	0.005544	0.710534
-29.776783	-1.872658	1.286234	0.005568	0.710528
-30.088535	-1.814628	1.291238	0.005626	0.710533
-29.791534	-1.870240	1.296243	0.005571	0.710528
-29.579491	-1.909852	1.301248	0.005531	0.710525
-29.809340	-1.953861	1.306253	0.005574	0.710356
-31.258689	-1.769390	1.311258	0.005843	0.710209
-30.508932	-1.899673	1.316262	0.005703	0.710216
-30.524456	-1.899550	1.321267	0.005706	0.710211
-31.150484	-1.789654	1.326272	0.005822	0.710208
-30.638333	-1.876147	1.331277	0.005727	0.710218
-30.697430	-1.870681	1.336282	0.005738	0.710208
-30.807679	-1.858912	1.341286	0.005758	0.710193
-31.205463	-1.941198	1.346291	0.005832	0.709887
-31.585859	-1.873395	1.351296	0.005902	0.709888
-31.963598	-1.803839	1.356301	0.005972	0.709893
-32.042728	-1.795386	1.361306	0.005987	0.709882
-31.404954	-1.905677	1.366310	0.005868	0.709889
-31.565268	-1.876120	1.371315	0.005897	0.709891
-32.016843	-1.797622	1.376320	0.005981	0.709888
-31.628519	-1.946447	1.381325	0.005909	0.709729
-32.547580	-1.852229	1.386330	0.006080	0.709591
-32.493567	-1.858643	1.391334	0.006069	0.709597
-32.540286	-1.852218	1.396339	0.006078	0.709594
-32.459965	-1.867496	1.401344	0.006063	0.709593
-32.266591	-1.900777	1.406349	0.006026	0.709595
-32.959991	-1.779882	1.411354	0.006155	0.709590
-32.788871	-1.876269	1.416358	0.006123	0.709459
-33.386832	-1.867993	1.421363	0.006234	0.709263
-33.367689	-1.873421	1.426368	0.006231	0.709259
-33.384381	-1.868056	1.431373	0.006233	0.709265
-33.395886	-1.870908	1.436378	0.006235	0.709255
-33.513965	-1.846186	1.441382	0.006257	0.709263
-33.479524	-1.853795	1.446387	0.006250	0.709260
-33.365264	-1.922196	1.451392	0.006229	0.709165
-34.277197	-1.864234	1.456397	0.006398	0.708956
-34.503820	-1.828628	1.461402	0.006440	0.708947
-34.361235	-1.850520	1.466406	0.006414	0.708954
-34.110178	-1.894357	1.471411	0.006367	0.708957
-34.518970	-1.824568	1.476416	0.006443	0.708951
-34.313113	-1.856762	1.481421	0.006404	0.708960
-34.154906	-1.910210	1.486426	0.006374	0.708910
-34.986310	-1.897382	1.491430	0.006529	0.708640
-35.238666	-1.853563	1.496435	0.006576	0.708638
-35.418630	-1.825451	1.501440	0.006609	0.708630
-34.734902	-1.941962	1.506445	0.006481	0.708641
-35.188943	-1.866249	1.511450	0.006566	0.708631
-35.385398	-1.828184	1.516454	0.006602	0.708638
-34.815810	-1.960474	1.521459	0.006496	0.708577
-35.697998	-1.918116	1.526464	0.006660	0.708347
-35.863013	-1.885305	1.531469	0.006690	0.708354
-36.199377	-1.831263	1.536474	0.006753	0.708343
-36.095928	-1.845016	1.541478	0.006733	0.708353
-35.927426	-1.876635	1.546483	0.006702	0.708350
-36.198720	-1.831036	1.551488	0.006752	0.708345
-35.890411	-1.945643	1.556493	0.006694	0.708226
-37.207803	-1.819696	1.561498	0.006939	0.708008
-36.727705	-1.903426	1.566502	0.006850	0.708012
-36.573944	-1.931717	1.571507	0.006821	0.708011
-37.278523	-1.809199	1.576512	0.006952	0.708005
-36.995929	-1.855274	1.581517	0.006899	0.708014
-36.646958	-1.921629	1.586522	0.006834	0.708006
-36.715921	-1.971922	1.591526	0.006846	0.707881
-37.911685	-1.850472	1.596531	0.007069	0.707698
-37.690825	-1.891618	1.601536	0.007027	0.707695
-37.269935	-1.962346	1.606541	0.006949	0.707704
-37.876421	-1.859371	1.611546	0.007061	0.707694
-37.980164	-1.837795	1.616550	0.007081	0.707701
-37.646922	-1.898738	1.621555	0.007018	0.707698
-37.898391	-1.939815	1.626560	0.007065	0.707526
-38.989208	-1.820371	1.631565	0.007268	0.707376
-38.740522	-1.867993	1.636570	0.007221	0.707370
-38.582937	-1.893193	1.641574	0.007192	0.707376
-38.625106	-1.885199	1.646579	0.007199	0.707378
-38.767304	-1.863187	1.651584	0.007225	0.707371
-38.312448	-1.939468	1.656589	0.007141	0.707381
-38.782164	-1.909871	1.661594	0.007228	0.707273
-39.713499	-1.838923	1.666598	0.007401	0.707083
-39.145285	-1.942606	1.671603	0.007295	0.707078
-39.737068	-1.840260	1.676608	0.007405	0.707073
-39.833493	-1.817658	1.681613	0.007423	0.707084
-39.465994	-1.887741	1.686618	0.007354	0.707075
-39.390290	-1.900486	1.691622	0.007340	0.707077
-39.675927	-1.893334	1.696627	0.007393	0.706990
-40.842089	-1.810561	1.701632	0.007609	0.706739
-40.065535	-1.942601	1.706637	0.007465	0.706752
-40.587500	-1.855222	1.711642	0.007562	0.706741
-40.780989	-1.817963	1.716646	0.007597	0.706747
-40.294379	-1.904808	1.721651	0.007507	0.706748
-40.536777	-1.864543	1.726656	0.007551	0.706742
-40.531275	-1.862171	1.731661	0.007550	0.706749
-40.951048	-1.930694	1.736666	0.007628	0.706462
-41.195659	-1.899898	1.741670	0.007673	0.706436
-41.251003	-1.890061	1.746675	0.007684	0.706437
-41.505945	-1.847324	1.751680	0.007731	0.706432
-41.076546	-1.920322	1.756685	0.007651	0.706439
-41.336391	-1.878498	1.761690	0.007699	0.706431
-41.528291	-1.842300	1.766694	0.007734	0.706435
-41.702688	-1.960900	1.771699	0.007767	0.706135
-42.009550	-1.915273	1.776704	0.007823	0.706117
-42.303902	-1.859298	1.781709	0.007878	0.706125
-42.345844	-1.855188	1.786714	0.007886	0.706118
-42.116696	-1.895250	1.791718	0.007843	0.706120
-42.072179	-1.903874	1.796723	0.007834	0.706119
-42.776306	-1.780170	1.801728	0.007965	0.706116
-42.322461	-1.969050	1.806733	0.007880	0.705899
-42.877449	-1.892848	1.811738	0.007983	0.705854
-43.222606	-1.830455	1.816742	0.008047	0.705856
-43.102372	-1.851218	1.821747	0.008025	0.705858
-43.170430	-1.842762	1.826752	0.008037	0.705851
-42.886859	-1.888917	1.831757	0.007984	0.705861
-43.377156	-1.805502	1.836762	0.008075	0.705853
-43.633303	-1.922044	1.841766	0.008123	0.705527
-43.578206	-1.936083	1.846771	0.008112	0.705519
-44.233720	-1.820574	1.851776	0.008234	0.705517
-43.590667	-1.931980	1.856781	0.008114	0.705524
-43.762629	-1.906124	1.861786	0.008146	0.705515
-44.267942	-1.813938	1.866790	0.008240	0.705519
-44.096376	-1.855529	1.871795	0.008208	0.705498
-44.872815	-1.863491	1.876800	0.008352	0.705203
-44.914069	-1.852095	1.881805	0.008359	0.705212
-45.387177	-1.771503	1.886810	0.008447	0.705205
-44.795352	-1.877038	1.891814	0.008337	0.705205
-44.789611	-1.877354	1.896819	0.008335	0.705207
-45.456184	-1.760877	1.901824	0.008459	0.705203
-44.831146	-1.869348	1.906829	0.008343	0.705209
-44.670668	-1.976176	1.911834	0.008313	0.705052
-46.136706	-1.798174	1.916838	0.008585	0.704885
-45.674970	-1.882806	1.921843	0.008499	0.704881
-45.830625	-1.857565	1.926848	0.008528	0.704876
-45.687602	-1.878402	1.931853	0.008501	0.704886
-45.987328	-1.829996	1.936858	0.008557	0.704876
-45.936470	-1.836806	1.941862	0.008547	0.704881
-45.710085	-1.935897	1.946867	0.008505	0.704763
-46.776030	-1.837161	1.951872	0.008703	0.704580
-46.352403	-1.907562	1.956877	0.008624	0.704590
-46.607667	-1.867467	1.961882	0.008671	0.704580
-46.721602	-1.845789	1.966886	0.008692	0.704583
-46.353592	-1.910149	1.971891	0.008623	0.704586
-46.582805	-1.872916	1.976896	0.008666	0.704579
-46.478658	-2.006843	1.981901	0.008646	0.704347
-47.731202	-1.831537	1.986906	0.008879	0.704251
-47.671265	-1.839851	1.991910	0.008868	0.704256
-46.956684	-1.966272	1.996915	0.008734	0.704259
-47.915853	-1.796332	2.001920	0.008913	0.704257

-47.418682	-1.886577	2.011917	0.008820	0.704255
-48.100978	-1.869950	2.021914	0.008946	0.704044
-48.157473	-1.909380	2.031910	0.008956	0.703945
-48.355265	-1.873515	2.041907	0.008993	0.703947
-48.467373	-1.854670	2.051904	0.009013	0.703945
-48.494667	-1.849900	2.061901	0.009018	0.703946
-47.997592	-1.830844	2.071898	0.008925	0.704164
-47.726980	-1.833757	2.081894	0.008874	0.704257
-47.605541	-1.854689	2.091891	0.008851	0.704259
-47.841799	-1.814757	2.101888	0.008894	0.704255
-47.593491	-1.860402	2.111885	0.008848	0.704253
-47.753316	-1.832003	2.121882	0.008877	0.704254
-47.368854	-1.901379	2.131878	0.008805	0.704253
-47.604203	-1.859090	2.141875	0.008848	0.704255
-47.168002	-1.840259	2.151872	0.008766	0.704451
-46.772027	-1.845140	2.161869	0.008692	0.704584
-46.795269	-1.842720	2.171866	0.008696	0.704581
-46.681357	-1.861418	2.181862	0.008674	0.704585
-46.753704	-1.848111	2.191859	0.008687	0.704587
-46.141743	-1.818198	2.201856	0.008573	0.704868
-45.687794	-1.893673	2.211853	0.008488	0.704880
-46.094255	-1.819910	2.221850	0.008563	0.704884
-45.967539	-1.843876	2.231846	0.008539	0.704882
-45.255895	-1.812494	2.241843	0.008406	0.705201
-44.988849	-1.856974	2.251840	0.008356	0.705208
-45.099233	-1.840652	2.261837	0.008376	0.705203
-45.092560	-1.807891	2.271834	0.008374	0.705272
-44.169255	-1.851355	2.281830	0.008202	0.705516
-43.867577	-1.904880	2.291827	0.008145	0.705518
-44.158148	-1.853758	2.301824	0.008199	0.705517
-43.909915	-1.820110	2.311821	0.008152	0.705675
-43.364452	-1.829210	2.321818	0.008050	0.705853
-43.016503	-1.890749	2.331814	0.007985	0.705855
-43.171191	-1.863696	2.341811	0.008013	0.705855
-42.651348	-1.862528	2.351808	0.007916	0.706045
-42.529874	-1.848284	2.361805	0.007893	0.706118
-42.370731	-1.876320	2.371802	0.007863	0.706119
-42.353652	-1.853297	2.381798	0.007859	0.706172
-41.819293	-1.819049	2.391795	0.007759	0.706434
-41.493103	-1.877912	2.401792	0.007698	0.706433
-41.748145	-1.834760	2.411789	0.007745	0.706429
-41.151496	-1.810631	2.421786	0.007634	0.706692
-40.643928	-1.876145	2.431782	0.007539	0.706743
-40.869559	-1.835359	2.441779	0.007580	0.706745
-40.382850	-1.838780	2.451776	0.007489	0.706914
-39.737525	-1.877148	2.461773	0.007368	0.707069
-39.997705	-1.831177	2.471770	0.007416	0.707069
-39.878024	-1.852098	2.481766	0.007394	0.707070
-39.289115	-1.814193	2.491763	0.007284	0.707358
-38.693500	-1.914533	2.501760	0.007172	0.707371
-39.221232	-1.821613	2.511757	0.007270	0.707369
-38.946881	-1.793685	2.521754	0.007218	0.707524
-38.074216	-1.866383	2.531750	0.007056	0.707691
-38.351873	-1.817611	2.541747	0.007107	0.707691
-38.031575	-1.848338	2.551744	0.007047	0.707745
-37.241194	-1.861670	2.561741	0.006899	0.708001
-37.195414	-1.869456	2.571738	0.006890	0.708003
-37.301717	-1.850213	2.581734	0.006909	0.708004
-36.875641	-1.822271	2.591731	0.006830	0.708213
-36.267709	-1.866295	2.601728	0.006716	0.708343
-36.586513	-1.812298	2.611725	0.006775	0.708338
-36.263676	-1.850899	2.621722	0.006714	0.708377
-35.601862	-1.843024	2.631718	0.006591	0.708630
-35.555182	-1.849487	2.641715	0.006581	0.708635
-35.604758	-1.840588	2.651712	0.006590	0.708636
-35.210159	-1.796046	2.661709	0.006516	0.708867
-34.711654	-1.844821	2.671706	0.006423	0.708948
-34.658492	-1.854037	2.681702	0.006413	0.708949
-34.547708	-1.827459	2.691699	0.006391	0.709043
-33.725729	-1.867605	2.701696	0.006238	0.709257
-34.141991	-1.793745	2.711693	0.006315	0.709257
-33.766776	-1.861296	2.721690	0.006245	0.709256
-33.229451	-1.806997	2.731686	0.006144	0.709558
-32.818677	-1.864473	2.741683	0.006067	0.709590
-33.018496	-1.829267	2.751680	0.006104	0.709590
-32.849413	-1.795057	2.761677	0.006072	0.709720
-32.066089	-1.852203	2.771674	0.005926	0.709885
-32.296331	-1.810091	2.781670	0.005968	0.709888
-32.039920	-1.848766	2.791667	0.005920	0.709903
-31.319276	-1.821630	2.801664	0.005785	0.710215
-31.571850	-1.779136	2.811661	0.005832	0.710211
-31.142563	-1.855576	2.821658	0.005751	0.710212
-31.012840	-1.776385	2.831654	0.005727	0.710417
-30.440684	-1.823980	2.841651	0.005620	0.710527
-30.396758	-1.831313	2.851648	0.005611	0.710529
-30.501422	-1.770456	2.861645	0.005630	0.710614
-29.409979	-1.840704	2.871642	0.005426	0.710863
-29.334470	-1.854447	2.881638	0.005412	0.710863
-29.343473	-1.852583	2.891635	0.005413	0.710865
-29.009305	-1.826366	2.901632	0.005350	0.711037
-28.626479	-1.846982	2.911629	0.005279	0.711133
-28.611306	-1.850757	2.921626	0.005275	0.711131
-28.614159	-1.830759	2.931622	0.005275	0.711171
-27.673029	-1.859850	2.941619	0.005100	0.711449
-27.775871	-1.841302	2.951616	0.005118	0.711450
-27.547637	-1.882182	2.961613	0.005076	0.711450
-27.495913	-1.805754	2.971610	0.005065	0.711622
-26.833478	-1.856826	2.981606	0.004942	0.711756
-26.953767	-1.834817	2.991603	0.004964	0.711758
-26.994690	-1.800922	3.001600	0.004971	0.711812
-26.100399	-1.824626	3.011597	0.004804	0.712084
-25.982974	-1.847171	3.021594	0.004781	0.712081
-25.938962	-1.853771	3.031590	0.004773	0.712085
-25.314063	-1.863389	3.041587	0.004656	0.712288
-25.423866	-1.797780	3.051584	0.004676	0.712381
-25.121740	-1.852372	3.061581	0.004619	0.712380
-25.073082	-1.829156	3.071578	0.004610	0.712445
-23.960826	-1.899099	3.081574	0.004402	0.712701
-23.965836	-1.898337	3.091571	0.004403	0.712701
-24.260064	-1.845807	3.101568	0.004457	0.712703
-23.994008	-1.817931	3.111565	0.004407	0.712853
-23.386633	-1.845551	3.121562	0.004293	0.713015
-23.505104	-1.824298	3.131558	0.004315	0.713016
-23.223558	-1.852483	3.141555	0.004262	0.713060
-22.655048	-1.807505	3.151552	0.004156	0.713352
-22.438913	-1.846812	3.161549	0.004115	0.713352
-22.513110	-1.833879	3.171546	0.004128	0.713352
-21.824420	-1.869675	3.181542	0.004000	0.713526
-21.549881	-1.858153	3.191539	0.003948	0.713647
-21.607170	-1.848823	3.201536	0.003958	0.713646
-21.344873	-1.896747	3.211533	0.003909	0.713644
-21.101337	-1.789846	3.221530	0.003863	0.713944
-20.731601	-1.846687	3.231526	0.003794	0.713963
-20.844058	-1.826506	3.241523	0.003814	0.713964
-20.266592	-1.829539	3.251520	0.003706	0.714163
-19.962542	-1.830573	3.261517	0.003649	0.714270
-19.931786	-1.836851	3.271514	0.003643	0.714269
-19.769576	-1.834837	3.281510	0.003612	0.714331
-18.962703	-1.841528	3.291507	0.003462	0.714604
-18.850421	-1.861228	3.301504	0.003440	0.714606
-18.783421	-1.874750	3.311501	0.003427	0.714604
-18.753890	-1.800306	3.321498	0.003421	0.714763
-17.690890	-1.919644	3.331494	0.003223	0.714903
-18.137146	-1.838973	3.341491	0.003306	0.714906
-17.929781	-1.877698	3.351488	0.003267	0.714903
-17.280324	-1.842908	3.361485	0.003145	0.715203
-16.964952	-1.888346	3.371482	0.003086	0.715225
-17.088634	-1.867624	3.381478	0.003109	0.715223
-17.131362	-1.802064	3.391475	0.003116	0.715339
-15.865023	-1.926421	3.401472	0.002880	0.715541
-16.111561	-1.884720	3.411469	0.002925	0.715537
-16.264894	-1.857258	3.421466	0.002953	0.715538
-15.395598	-1.912705	3.431462	0.002791	0.715736
-15.293087	-1.858501	3.441459	0.002771	0.715881
-14.979774	-1.915902	3.451456	0.002713	0.715878
-15.206682	-1.875413	3.461453	0.002754	0.715879
-14.541561	-1.901614	3.471450	0.002630	0.716063
-14.346019	-1.905570	3.481446	0.002593	0.716125
-14.527280	-1.872739	3.491443	0.002626	0.716127
-14.368415	-1.856191	3.501440	0.002596	0.716217
-13.488893	-1.899815	3.511437	0.002432	0.716442
-13.465619	-1.904800	3.521434	0.002427	0.716441
-13.314672	-1.929843	3.531430	0.002399	0.716445
-13.073699	-1.861301	3.541427	0.002354	0.716667
-12.672187	-1.890229	3.551424	0.002278	0.716752
-12.823981	-1.864226	3.561421	0.002306	0.716751
-12.452541	-1.878037	3.571418	0.002236	0.716855
-11.638851	-1.910967	3.581414	0.002085	0.717078
-11.628222	-1.912159	3.591411	0.002082	0.717080
-11.647179	-1.908437	3.601408	0.002085	0.717082
-11.272133	-1.861536	3.611405	0.002015	0.717308
-10.989214	-1.878979	3.621402	0.001962	0.717374
-10.626014	-1.943998	3.631398	0.001894	0.717374
-10.819416	-1.866042	3.641395	0.001929	0.717461
-9.659448	-1.951805	3.651392	0.001713	0.717700
-10.041484	-1.885943	3.661389	0.001783	0.717697
-9.802994	-1.928392	3.671386	0.001739	0.717698
-9.742969	-1.842282	3.681382	0.001727	0.717890
-9.045278	-1.904497	3.691379	0.001596	0.718014
-9.044125	-1.903920	3.701376	0.001596	0.718016
-9.034117	-1.879206	3.711373	0.001593	0.718069
-8.035878	-1.915546	3.721370	0.001407	0.718349
-8.016547	-1.919987	3.731366	0.001403	0.718348
-7.960201	-1.928607	3.741363	0.001392	0.718352
-7.715235	-1.914891	3.751360	0.001346	0.718466
-7.256386	-1.910791	3.761357	0.001260	0.718636
-7.218649	-1.917759	3.771354	0.001253	0.718637
-7.447398	-1.876630	3.781350	0.001295	0.718638
-6.583921	-1.883140	3.791347	0.001134	0.718930
-6.318498	-1.917190	3.801344	0.001084	0.718957
-6.301162	-1.921316	3.811341	0.001080	0.718956
-6.337837	-1.861230	3.821338	0.001086	0.719062
-5.621108	-1.888079	3.831334	0.000952	0.719262
-5.276971	-1.948307	3.841331	0.000888	0.719265
-5.262993	-1.949695	3.851328	0.000885	0.719268
-5.042350	-1.862352	3.861325	0.000843	0.719519
-4.570568	-1.909389	3.871322	0.000755	0.719592
-4.533112	-1.916147	3.881318	0.000747	0.719593
-4.466696	-1.884325	3.891315	0.000735	0.719680
-3.722642	-1.908723	3.901312	0.000596	0.719894
-3.675351	-1.917827	3.911309	0.000586	0.719893
-3.529580	-1.944826	3.921306	0.000559	0.719892
-3.365897	-1.860079	3.931302	0.000528	0.720117
-2.907717	-1.888743	3.941299	0.000442	0.720222
-2.824982	-1.904358	3.951296	0.000426	0.720222
-2.689666	-1.887424	3.961293	0.000401	0.720303
-2.228696	-1.852452	3.971290	0.000314	0.720535
-2.237924	-1.850459	3.981286	0.000315	0.720536
-2.238103	-1.833004	3.991283	0.000315	0.720571
-1.885439	-1.742075	4.001280	0.000249	0.720875
-1.776782	-1.762821	4.011277	0.000228	0.720873
-1.760277	-1.732557	4.021274	0.000225	0.720939
-1.484883	-1.693081	4.031270	0.000173	0.721114
-1.544774	-1.681469	4.041267	0.000183	0.721117
-1.182928	-1.618966	4.051264	0.000116	0.721367
-1.255445	-1.574098	4.061261	0.000129	0.721431
-1.111588	-1.525014	4.071258	0.000101	0.721579
-0.975552	-1.468316	4.081254	0.000075	0.721739
-1.021180	-1.385896	4.091251	0.000083	0.721885
-0.798679	-1.331309	4.101248	0.000042	0.722071
-0.861020	-1.237282	4.111245	0.000053	0.722235
-0.976633	-1.152938	4.121242	0.000074	0.722361
-0.930564	-1.016978	4.131238	0.000065	0.722645
-0.894106	-0.950275	4.141235	0.000057	0.722789
-0.728240	-0.872375	4.151232	0.000026	0.723001
-0.656002	-0.739352	4.161229	0.000012	0.723288
-0.726197	-0.637327	4.171226	0.000024	0.723464
-0.530568	-0.569888	4.181222	-0.000013	0.723666
-0.347379	-0.457998	4.191219	-0.000047	0.723950
-0.337334	-0.333543	4.201216	-0.000050	0.724198
-0.385635	-0.202090	4.211213	-0.000041	0.724439
-0.421979	-0.065576	4.221210	-0.000035	0.724695
-0.405445	0.066323	4.231206	-0.000039	0.724959
0.000000	0.183933	4.241203	-0.000115	0.725331

-0.308306	0.850113	4.246208	-0.000058	0.726526
-0.071366	2.084245	4.251213	-0.000103	0.729013
0.259226	3.896441	4.256218	-0.000166	0.732644
0.397221	6.288112	4.261222	-0.000194	0.737307
0.763245	9.160184	4.266227	-0.000264	0.742935
0.811016	12.560541	4.271232	-0.000275	0.749414
1.288918	16.341515	4.276237	-0.000367	0.756694
1.442009	20.581462	4.281242	-0.000398	0.764650
1.812821	25.188970	4.286246	-0.000471	0.773269
2.402408	30.124994	4.291251	-0.000584	0.782458
2.579523	35.475409	4.296256	-0.000621	0.792152
2.802247	41.135263	4.301261	-0.000666	0.802290
3.490049	47.015260	4.306266	-0.000798	0.812829
4.032787	53.205999	4.311270	-0.000903	0.823723
4.479688	59.701144	4.316275	-0.000991	0.834964
5.054282	66.370486	4.321280	-0.001103	0.846384
5.624706	73.285186	4.326285	-0.001214	0.858057
6.288707	80.391934	4.331290	-0.001342	0.869912
6.553417	87.731238	4.336294	-0.001396	0.881869
7.124823	95.214769	4.341299	-0.001508	0.893979
7.853114	102.807351	4.346304	-0.001649	0.906142
8.348992	110.603228	4.351309	-0.001746	0.918394
9.077362	118.460105	4.356314	-0.001887	0.930639
9.435865	126.494953	4.361318	-0.001960	0.942895
10.748145	134.483274	4.366323	-0.002209	0.955171
12.491963	142.485277	4.371328	-0.002539	0.967422
13.495447	150.728212	4.376333	-0.002732	0.979680
14.200883	159.122694	4.381338	-0.002869	0.991929
15.142886	167.493988	4.386342	-0.003050	1.004053
16.063431	175.936627	4.391347	-0.003227	1.016126
16.641697	184.460984	4.396352	-0.003341	1.028088
17.303195	193.019999	4.401357	-0.003470	1.039979
18.192647	201.568124	4.406362	-0.003641	1.051773
18.738796	210.187573	4.411366	-0.003749	1.063452
19.305769	218.859229	4.416371	-0.003860	1.075078
19.771697	227.501508	4.421376	-0.003953	1.086517
20.545710	236.127091	4.426381	-0.004103	1.097884
21.559320	244.711337	4.431386	-0.004297	1.109134
22.223452	253.358012	4.436390	-0.004427	1.120274
22.909687	262.004320	4.441395	-0.004560	1.131308
23.190819	270.704361	4.446400	-0.004619	1.142215
24.163398	279.320129	4.451405	-0.004806	1.153061
24.682373	287.967348	4.456410	-0.004908	1.163749
25.293144	296.586401	4.461414	-0.005028	1.174325
25.974564	305.187239	4.466419	-0.005160	1.184798
26.499584	313.810008	4.471424	-0.005264	1.195174
27.470288	322.331831	4.476429	-0.005450	1.205431
28.361155	330.880746	4.481434	-0.005622	1.215616
29.059943	339.433307	4.486438	-0.005758	1.225683
29.561994	348.052447	4.491443	-0.005857	1.235705
29.924107	356.615175	4.496448	-0.005931	1.245556
30.569561	365.143728	4.501453	-0.006057	1.255344
31.175811	373.657470	4.506458	-0.006175	1.265033
31.829728	382.166139	4.511462	-0.006303	1.274651
32.611058	390.634234	4.516467	-0.006454	1.284175
32.919555	399.169363	4.521472	-0.006517	1.293616
33.386543	407.657273	4.526477	-0.006610	1.302965
34.013969	416.198150	4.531482	-0.006733	1.312334
34.612425	424.647249	4.536486	-0.006850	1.321532
35.204067	433.057188	4.541491	-0.006966	1.330624
35.529102	441.493040	4.546496	-0.007032	1.339634
36.043778	449.890247	4.551501	-0.007133	1.348576
36.717837	458.268992	4.556506	-0.007265	1.357468
36.808978	466.692420	4.561510	-0.007287	1.366247
37.190915	475.098571	4.566515	-0.007364	1.375002
37.991208	483.402247	4.571520	-0.007519	1.383667
38.896862	491.728122	4.576525	-0.007693	1.392319
39.310237	500.099621	4.581530	-0.007776	1.400881
39.733789	508.447124	4.586534	-0.007860	1.409368
40.412365	516.771446	4.591539	-0.007992	1.417823
40.917974	525.082213	4.596544	-0.008092	1.426186
41.266042	533.456862	4.601549	-0.008163	1.434537
41.697987	541.772633	4.606554	-0.008249	1.442795
41.867675	550.128416	4.611558	-0.008286	1.451004
42.574674	558.401705	4.616563	-0.008423	1.459171
43.040657	566.698089	4.621568	-0.008516	1.467277
43.690622	575.024871	4.626573	-0.008642	1.475397
44.089836	583.305649	4.631578	-0.008722	1.483388
44.437867	591.590098	4.636582	-0.008793	1.491332
45.109743	599.842879	4.641587	-0.008923	1.499254
45.562932	608.107338	4.646592	-0.009013	1.507112
45.852677	616.413166	4.651597	-0.009073	1.514942
46.292479	624.671697	4.656602	-0.009161	1.522710
47.093637	632.857434	4.661606	-0.009315	1.530427
47.880368	641.083137	4.666611	-0.009467	1.538138
48.220831	649.339028	4.671616	-0.009536	1.545772
48.614440	657.637539	4.676621	-0.009615	1.553416
49.058695	665.871035	4.681626	-0.009704	1.560970
49.443505	674.102756	4.686630	-0.009781	1.568477
49.839477	682.364992	4.691635	-0.009860	1.575978
50.274844	690.574207	4.696640	-0.009947	1.583401
50.581352	698.830984	4.701645	-0.010010	1.590813
50.815942	707.091392	4.706650	-0.010059	1.598183
51.365740	715.255593	4.711654	-0.010167	1.605480
51.979896	723.474672	4.716659	-0.010287	1.612800
52.297181	731.689220	4.721664	-0.010351	1.620042
52.835608	739.884754	4.726669	-0.010457	1.627265
53.249275	748.157833	4.731674	-0.010540	1.634507
53.722567	756.319262	4.736678	-0.010634	1.641628
54.157241	764.509407	4.741683	-0.010720	1.648737
54.479176	772.712855	4.746688	-0.010786	1.655812
54.640874	780.929973	4.751693	-0.010821	1.662847
55.244464	789.098695	4.756698	-0.010939	1.669870
55.477913	797.300571	4.761702	-0.010988	1.676843
56.006615	805.458378	4.766707	-0.011092	1.683788
56.300244	813.652059	4.771712	-0.011153	1.690704
56.781557	821.829221	4.776717	-0.011248	1.697602
57.388790	829.980865	4.781722	-0.011366	1.704468
57.743702	838.182421	4.786726	-0.011438	1.711314
57.971147	846.398843	4.791731	-0.011486	1.718129
58.377482	854.534470	4.796736	-0.011567	1.724873
58.923711	862.689978	4.801741	-0.011674	1.731625
59.171101	870.889315	4.806746	-0.011726	1.738348
59.507791	879.027630	4.811750	-0.011794	1.745007
60.162021	887.174205	4.816755	-0.011922	1.751688
60.543428	895.336254	4.821760	-0.011998	1.758321
61.028119	903.455634	4.826765	-0.012094	1.764908
61.500867	911.632332	4.831770	-0.012188	1.771514
61.607030	919.823580	4.836774	-0.012213	1.778062
61.753403	928.019632	4.841779	-0.012246	1.784594
62.200718	936.185363	4.846784	-0.012335	1.791116
62.578626	944.349470	4.851789	-0.012410	1.797604
62.737092	952.505435	4.856794	-0.012446	1.804035
63.070720	960.624284	4.861798	-0.012513	1.810436
63.712712	968.744031	4.866803	-0.012638	1.816852
63.936427	976.884449	4.871808	-0.012685	1.823211
64.056702	985.057559	4.876813	-0.012713	1.829561
64.765033	993.151547	4.881818	-0.012851	1.835897
64.965895	1001.290600	4.886822	-0.012894	1.842186
65.256509	1009.453291	4.891827	-0.012953	1.848483
65.782520	1017.559981	4.896832	-0.013057	1.854743
66.350743	1025.657535	4.901837	-0.013168	1.860979
66.907647	1033.778147	4.906842	-0.013277	1.867211
67.088035	1041.975011	4.911846	-0.013317	1.873436
67.507860	1050.098164	4.916851	-0.013400	1.879612
67.829770	1058.207826	4.921856	-0.013466	1.885747
68.099951	1066.369810	4.926861	-0.013522	1.891895
68.547114	1074.483600	4.931866	-0.013610	1.898006
68.805758	1082.599641	4.936870	-0.013664	1.904079
69.031451	1090.759055	4.941875	-0.013712	1.910161
69.401565	1098.878268	4.946880	-0.013786	1.916209
69.922347	1106.959601	4.951885	-0.013889	1.922228
70.286188	1115.095096	4.956890	-0.013962	1.928250
70.632271	1123.231309	4.961894	-0.014032	1.934251
70.828785	1131.379675	4.966899	-0.014074	1.940227
71.009564	1139.504208	4.971904	-0.014113	1.946165
71.409066	1147.653419	4.976909	-0.014193	1.952126
72.016669	1155.733015	4.981914	-0.014312	1.958041
72.342856	1163.810828	4.986918	-0.014378	1.963907
72.697817	1171.919869	4.991923	-0.014449	1.969781
73.124225	1180.020110	4.996928	-0.014534	1.975638
73.392903	1188.134632	5.001933	-0.014590	1.981472
73.831570	1196.226087	5.006938	-0.014677	1.987290
74.052572	1204.359718	5.011942	-0.014724	1.993098
74.586067	1212.448389	5.016947	-0.014829	1.998889
74.806122	1220.539807	5.021952	-0.014875	2.004633
75.159131	1228.658450	5.026957	-0.014946	2.010394
75.610836	1236.765634	5.031962	-0.015036	2.016140
75.706876	1244.883085	5.036966	-0.015059	2.021840
75.980242	1253.018185	5.041971	-0.015116	2.027555
76.338795	1261.134103	5.046976	-0.015188	2.033249
76.828043	1269.199881	5.051981	-0.015285	2.038905
77.434090	1277.252367	5.056986	-0.015403	2.044549
77.543182	1285.383334	5.061990	-0.015429	2.050180
77.873590	1293.501162	5.066995	-0.015496	2.055809
78.121870	1301.595785	5.072000	-0.015548	2.061399
78.344582	1309.702881	5.077005	-0.015595	2.066979
78.879882	1317.786692	5.082010	-0.015700	2.072560
79.150613	1325.873981	5.087014	-0.015756	2.078102
79.472699	1333.974696	5.092019	-0.015821	2.083642
79.871678	1342.052422	5.097024	-0.015901	2.089161
80.292741	1350.160414	5.102029	-0.015985	2.094687
80.639948	1358.256155	5.107034	-0.016055	2.100183
80.907964	1366.337002	5.112038	-0.016111	2.105646
81.312487	1374.490362	5.117043	-0.016191	2.111158
81.590881	1382.618889	5.122048	-0.016249	2.116626
81.603022	1390.713647	5.127053	-0.016257	2.122032
81.898284	1398.794415	5.132058	-0.016317	2.127442
82.339135	1406.847768	5.137062	-0.016405	2.132834
82.388602	1414.974036	5.142067	-0.016419	2.138223
82.375510	1423.069763	5.147072	-0.016422	2.143573
82.805400	1431.126087	5.152077	-0.016508	2.148925
83.406404	1439.212116	5.157082	-0.016625	2.154299
83.604772	1447.264794	5.162086	-0.016668	2.159600
83.986258	1455.344270	5.167091	-0.016744	2.164923
84.098353	1463.438476	5.172096	-0.016771	2.170217
84.722064	1471.485553	5.177101	-0.016892	2.175515
85.231215	1479.549745	5.182106	-0.016993	2.180800
85.537311	1487.626509	5.187110	-0.017055	2.186062
85.870028	1495.756680	5.192115	-0.017123	2.191348
86.167486	1503.859382	5.197120	-0.017183	2.196601
86.494026	1511.918814	5.202125	-0.017250	2.201815
86.846926	1519.993402	5.207130	-0.017321	2.207030
87.186178	1528.075367	5.212134	-0.017390	2.212235
87.654214	1536.153626	5.217139	-0.017482	2.217438
87.970784	1544.203814	5.222144	-0.017547	2.222596
88.067898	1552.323143	5.227149	-0.017570	2.227767
88.299942	1560.442034	5.232154	-0.017619	2.232938
88.586874	1568.492485	5.237158	-0.017678	2.238058
88.966267	1576.552391	5.242163	-0.017754	2.243181
89.006165	1584.661978	5.247168	-0.017767	2.248293
89.326371	1592.745560	5.252173	-0.017832	2.253402
89.487960	1600.842125	5.257178	-0.017868	2.258493
89.700159	1608.900856	5.262182	-0.017913	2.263554
90.033931	1616.978450	5.267187	-0.017980	2.268626
90.385965	1625.115496	5.272192	-0.018051	2.273725
90.595520	1633.160518	5.277197	-0.018096	2.278743
91.102137	1641.183422	5.282202	-0.018196	2.283761
91.470824	1649.204970	5.287206	-0.018270	2.288756
91.683461	1657.318191	5.292211	-0.018315	2.293783
91.912398	1665.392847	5.297216	-0.018363	2.298777
92.114684	1673.454318	5.302221	-0.018406	2.303750
92.520832	1681.531141	5.307226	-0.018487	2.308738
93.013560	1689.577616	5.312230	-0.018585	2.313704
93.287517	1697.650658	5.317235	-0.018641	2.318658
93.674212	1705.686285	5.322240	-0.018718	2.323587
93.858655	1713.776588	5.327245	-0.018758	2.328522
94.132005	1721.884710	5.332250	-0.018815	2.333465
94.337025	1729.940030	5.337254	-0.018858	2.338360
94.769761	1738.000608	5.342259	-0.018944	2.343266
94.963278	1746.082562	5.347264	-0.018986	2.348156
95.018081	1754.215080	5.352269	-0.019002	2.353054
95.321513	1762.276607	5.357274	-0.019064	2.357920
95.782840	1770.276848	5.362278	-0.019155	2.362751
95.720168	1778.394967	5.367283	-0.019149	2.367601
96.091906	1786.433808	5.372288	-0.019224	2.372429
96.313025	1794.515030	5.377293	-0.019270	2.377259
96.612059	1802.566116	5.382298	-0.019331	2.382069
96.760360	1810.617523	5.387302	-0.019365	2.386857
97.198467	1818.693159	5.392307	-0.019452	2.391672
97.370018	1826.770989	5.397312	-0.019489	2.396458
97.629182	1834.815509	5.402317	-0.019543	2.401221
98.128761	1842.850537	5.407322	-0.019641	2.405989
98.317741	1850.920799	5.412326	-0.019682	2.410743
98.435002	1859.023050	5.417331	-0.019709	2.415501
98.650094	1867.073096	5.422336	-0.019755	2.420226
98.945799	1875.109619	5.427341	-0.019815	2.424941
99.200716	1883.205459	5.432346	-0.019868	2.429678
99.330136	1891.353457	5.437350	-0.019898	2.434426
99.803660	1899.364682	5.442355	-0.019992	2.439112
99.880730	1907.417108	5.447360	-0.020011	2.443783
100.002340	1915.474552	5.452365	-0.020040	2.448451
100.243484	1923.545584	5.457370	-0.020090	2.453126
100.578857	1931.566390	5.462374	-0.020158	2.457771
100.835922	1939.622898	5.467379	-0.020211	2.462422
101.178661	1947.659111	5.472384	-0.020280	2.467059
101.340772	1955.750606	5.477389	-0.020316	2.471705
101.567366	1963.815146	5.482394	-0.020364	2.476332
101.710989	1971.852041	5.487398	-0.020396	2.480928
102.264135	1979.865298	5.492403	-0.020505	2.485533
102.385590	1987.948104	5.497408	-0.020533	2.490136
102.729956	1996.019296	5.502413	-0.020602	2.494741
102.993325	2004.069200	5.507418	-0.020657	2.499319
103.280746	2012.096109	5.512422	-0.020716	2.503878
103.599838	2020.198550	5.517427	-0.020781	2.508473
103.845700	2028.284150	5.522432	-0.020832	2.513045
104.113718	2036.330655	5.527437	-0.020887	2.517588
104.333227	2044.385567	5.532442	-0.020934	2.522124
104.388588	2052.437108	5.537446	-0.020949	2.526638
104.673973	2060.506920	5.542451	-0.021008	2.531171
104.986585	2068.559637	5.547456	-0.021072	2.535688
105.129509	2076.601445	5.552461	-0.021104	2.540179
105.736486	2084.616757	5.557466	-0.021222	2.544680
105.802053	2092.698026	5.562470	-0.021240	2.549171
105.993527	2100.794813	5.567475	-0.021281	2.553672
106.304677	2108.830974	5.572480	-0.021345	2.558140
106.574500	2116.863416	5.577485	-0.021400	2.562595
107.043212	2124.905569	5.582490	-0.021493	2.567061
107.083241	2132.970398	5.587494	-0.021506	2.571503
107.479394	2141.050987	5.592499	-0.021585	2.575969
107.808765	2149.079613	5.597504	-0.021652	2.580395
108.004064	2157.123944	5.602509	-0.021694	2.584813
108.216904	2165.209123	5.607514	-0.021739	2.589246
108.415686	2173.444933	5.612518	-0.021782	2.593754
108.916810	2181.440842	5.617523	-0.021880	2.598143
109.011439	2189.418842	5.622528	-0.021903	2.602487
109.241435	2197.426472	5.627533	-0.021952	2.606850
109.491883	2205.481732	5.632538	-0.022004	2.611232
109.647034	2213.529598	5.637542	-0.022038	2.615596
109.882674	2221.552679	5.642547	-0.022088	2.619945
110.234792	2229.568447	5.647552	-0.022159	2.624291
110.360728	2237.632355	5.652557	-0.022188	2.628640
110.694263	2245.695128	5.657562	-0.022255	2.632995
110.954463	2253.729829	5.662566	-0.022309	2.637323
111.185322	2261.786752	5.667571	-0.022358	2.641654
110.924854	2269.866851	5.672576	-0.022315	2.645958
111.402952	2277.877288	5.677581	-0.022409	2.650266
111.617365	2285.962060	5.682586	-0.022454	2.654590
111.822878	2293.984905	5.687590	-0.022498	2.658872
112.236869	2302.017719	5.692595	-0.022581	2.663167
112.469615	2310.059330	5.697600	-0.022630	2.667447
112.442891	2318.153832	5.702605	-0.022630	2.671732
112.771344	2326.231772	5.707610	-0.022697	2.676025
113.048471	2334.213095	5.712614	-0.022754	2.680255
113.333589	2342.239430	5.717619	-0.022812	2.684504
113.509817	2350.313194	5.722624	-0.022851	2.688764
113.879454	2358.349769	5.727629	-0.022925	2.693009
114.118853	2366.417921	5.732634	-0.022975	2.697256
114.249874	2374.432627	5.737638	-0.023005	2.701462
114.555974	2382.489670	5.742643	-0.023067	2.705694
114.716306	2390.539289	5.747648	-0.023103	2.709907
114.909190	2398.618618	5.752653	-0.023144	2.714130
115.284843	2406.635377	5.757658	-0.023219	2.718326
115.471690	2414.665630	5.762662	-0.023260	2.722510
115.620345	2422.720731	5.767667	-0.023293	2.726699
115.795010	2430.784615	5.772672	-0.023331	2.730887
116.296202	2438.821010	5.777677	-0.023430	2.735074
116.378166	2446.873128	5.782682	-0.023450	2.739238
116.355781	2454.922029	5.787686	-0.023452	2.743387
116.898885	2462.956351	5.792691	-0.023558	2.747557
117.434881	2471.019230	5.797696	-0.023664	2.751734
117.606000	2479.123035	5.802701	-0.023701	2.755904
117.892310	2487.130579	5.807706	-0.023760	2.760026
118.131450	2495.115505	5.812710	-0.023810	2.764127
118.448274	2503.166307	5.817715	-0.023874	2.768259
118.596781	2511.237383	5.822720	-0.023907	2.772386
118.728452	2519.279616	5.827725	-0.023937	2.776492
118.975189	2527.332088	5.832730	-0.023989	2.780603
119.301449	2535.325246	5.837734	-0.024055	2.784682
119.532300	2543.403002	5.842739	-0.024103	2.788793
119.602436	2551.470125	5.847744	-0.024122	2.792883
119.695623	2559.508149	5.852749	-0.024145	2.796953
120.033809	2567.525905	5.857754	-0.024213	2.801022
120.259654	2575.544318	5.862758	-0.024261	2.805078
120.740983	2583.574820	5.867763	-0.024356	2.809150
120.918078	2591.644165	5.872768	-0.024394	2.813217
121.117864	2599.686596	5.877773	-0.024437	2.817266
121.478162	2607.734159	5.882778	-0.024510	2.821321
121.579972	2615.756310	5.887782	-0.024534	2.825343
122.049620	2623.811683	5.892787	-0.024627	2.829397
122.358277	2631.901620	5.897792	-0.024690	2.833452
122.447835	2639.921090	5.902797	-0.024712	2.837455
122.955055	2647.942132	5.907802	-0.024812	2.841476
122.995914	2655.956709	5.912806	-0.024825	2.845462
123.110132	2664.015160	5.917811	-0.024852	2.849468
123.294311	2672.096653	5.922816	-0.024891	2.853484
123.589029	2680.115933	5.927821	-0.024952	2.857469
124.177223	2688.130578	5.932826	-0.025067	2.861463
124.274233	2696.146802	5.937830	-0.025090	2.865425
124.469429	2704.205627	5.942835	-0.025132	2.869408
124.658937	2712.291636	5.947840	-0.025173	2.873398
124.705175	2720.322393	5.952845	-0.025187	2.877348
124.840580	2728.364443	5.957850	-0.025218	2.881302
124.998778	2736.387673	5.962854	-0.025253	2.885244
125.398172	2744.436606	5.967859	-0.025332	2.889205
125.527811	2752.490356	5.972864	-0.025362	2.893149
125.931941	2760.503603	5.977869	-0.025443	2.897082
126.114547	2768.570443	5.982874	-0.025482	2.901024
126.209974	2776.586121	5.987878	-0.025505	2.904932
126.578050	2784.626907	5.992883	-0.025579	2.908860
126.826982	2792.726001	5.997888	-0.025631	2.912806
127.092908	2800.760246	6.002893	-0.025686	2.916715
127.167448	2808.807713	6.007898	-0.025706	2.920615
127.193736	2816.793739	6.012902	-0.025716	2.924478
127.513994	2824.832597	6.017907	-0.025781	2.928377
127.642993	2832.889623	6.022912	-0.025811	2.932269
127.773035	2840.933316	6.027917	-0.025840	2.936150
128.133313	2848.938000	6.032922	-0.025913	2.940019
128.339055	2856.925329	6.037926	-0.025957	2.943866
128.448641	2865.004635	6.042931	-0.025983	2.947747
128.654791	2873.066601	6.047936	-0.026026	2.951620
129.120183	2881.076666	6.052941	-0.026118	2.955476
129.514194	2889.103182	6.057946	-0.026197	2.959332
129.656762	2897.115719	6.062950	-0.026229	2.963162
130.096682	2905.150689	6.067955	-0.026317	2.967014
130.441737	2913.200605	6.072960	-0.026386	2.970863
130.334130	2921.297768	6.077965	-0.026372	2.974706
130.649037	2929.323360	6.082970	-0.026436	2.978532
130.815255	2937.330491	6.087974	-0.026472	2.982336
131.066118	2945.394357	6.092979	-0.026525	2.986167
131.342878	2953.428308	6.097984	-0.026582	2.989980
131.553436	2961.495565	6.102989	-0.026626	2.993800
131.793419	2969.513168	6.107994	-0.026676	2.997594
131.888454	2977.535818	6.112998	-0.026700	3.001378
132.356356	2985.543933	6.118003	-0.026792	3.005168
132.383001	2993.607534	6.123008	-0.026803	3.008958
132.659777	3001.625750	6.128013	-0.026860	3.012735
132.865544	3009.669624	6.133018	-0.026903	3.016515
133.056129	3017.687252	6.138022	-0.026944	3.020277
133.592988	3025.679469	6.143027	-0.027050	3.024040
133.684187	3033.739114	6.148032	-0.027072	3.027807
133.964071	3041.789881	6.153037	-0.027130	3.031575
134.064122	3049.887612	6.158042	-0.027154	3.035352
134.142359	3057.870824	6.163046	-0.027174	3.039069
134.458090	3065.900461	6.168051	-0.027238	3.042815
134.489788	3073.954027	6.173056	-0.027250	3.046554
134.647985	3081.984916	6.178061	-0.027285	3.050283
134.993288	3090.038859	6.183066	-0.027354	3.054028
135.090727	3098.070903	6.188070	-0.027378	3.057746
135.080115	3106.127919	6.193075	-0.027381	3.061465
135.441602	3114.124140	6.198080	-0.027454	3.065170
135.715553	3122.144596	6.203085	-0.027511	3.068878
136.060027	3130.248512	6.208090	-0.027580	3.072622
136.100437	3138.316619	6.213094	-0.027593	3.076332
136.469735	3146.288938	6.218099	-0.027667	3.080008
136.526468	3154.300619	6.223104	-0.027684	3.083683
136.469583	3162.340896	6.228109	-0.027678	3.087362
136.966284	3170.365577	6.233114	-0.027776	3.091054
137.240694	3178.389691	6.238118	-0.027833	3.094732
137.336540	3186.457895	6.243123	-0.027856	3.098417
137.395344	3194.468868	6.248128	-0.027873	3.102070
137.593973	3202.486291	6.253133	-0.027915	3.105728
137.727360	3210.547288	6.258138	-0.027945	3.109399
137.742789	3218.604204	6.263142	-0.027954	3.113058
138.067303	3226.639823	6.268147	-0.028020	3.116717
138.253697	3234.642242	6.273152	-0.028060	3.120350
138.421059	3242.640789	6.278157	-0.028096	3.123977
138.716126	3250.676166	6.283162	-0.028157	3.127621
138.792290	3258.716412	6.288166	-0.028176	3.131254
139.004961	3266.771282	6.293171	-0.028222	3.134895
139.267810	3274.793929	6.298176	-0.028276	3.138520
139.500144	3282.810932	6.303181	-0.028325	3.142136
139.745498	3290.839496	6.308186	-0.028376	3.145755
139.862511	3298.881642	6.313190	-0.028403	3.149369
140.150288	3306.941501	6.318195	-0.028462	3.152994
140.489091	3314.970234	6.323200	-0.028531	3.156604
140.462314	3323.001293	6.328205	-0.028531	3.160195
140.875502	3330.993870	6.333210	-0.028614	3.163783
141.151154	3339.007661	6.338214	-0.028670	3.167371
141.373196	3347.049885	6.343219	-0.028717	3.170965
141.474884	3355.140332	6.348224	-0.028742	3.174571
141.598979	3363.157798	6.353229	-0.028770	3.178142
141.783971	3371.182717	6.358234	-0.028810	3.181714
141.882252	3379.213807	6.363238	-0.028834	3.185282
142.335185	3387.231990	6.368243	-0.028924	3.188855
142.574727	3395.293192	6.373248	-0.028974	3.192433
142.785790	3403.313298	6.378253	-0.029018	3.195989
143.053308	3411.330712	6.383258	-0.029074	3.199541
143.207298	3419.354503	6.388262	-0.029108	3.203088
143.490113	3427.391366	6.393267	-0.029166	3.206642
143.727477	3435.416046	6.398272	-0.029216	3.210184
143.958991	3443.461633	6.403277	-0.029264	3.213732
144.035066	3451.515935	6.408282	-0.029284	3.217273
144.046181	3459.536846	6.413286	-0.029291	3.220793
144.487393	3467.531915	6.418291	-0.029379	3.224315
144.841355	3475.563380	6.423296	-0.029450	3.227845
144.927352	3483.615987	6.428301	-0.029472	3.231370
145.123308	3491.730833	6.433306	-0.029514	3.234923
145.122165	3499.694783	6.438310	-0.029519	3.238398
145.402872	3507.719968	6.443315	-0.029577	3.241908
145.494417	3515.706943	6.448320	-0.029599	3.245389
145.801314	3523.708501	6.453325	-0.029662	3.248882
146.163606	3531.777707	6.458330	-0.029735	3.252402
146.232130	3539.841128	6.463334	-0.029753	3.255904
146.356646	3547.838960	6.468339	-0.029782	3.259377
146.614013	3555.863510	6.473344	-0.029835	3.262862
146.910884	3563.888828	6.478349	-0.029896	3.266346
147.219330	3571.926871	6.483354	-0.029959	3.269831
147.485393	3579.944220	6.488358	-0.030014	3.273303
147.883245	3587.992291	6.493363	-0.030093	3.276789
147.808177	3596.021666	6.498368	-0.030085	3.280244
148.024722	3604.021484	6.503373	-0.030131	3.283695
148.289550	3612.092327	6.508378	-0.030185	3.287175
148.498647	3620.079397	6.513382	-0.030230	3.290612
148.650199	3628.144912	6.518387	-0.030263	3.294078
149.131847	3636.155135	6.523392	-0.030359	3.297529
149.206337	3644.183423	6.528397	-0.030378	3.300968
149.566299	3652.203403	6.533402	-0.030450	3.304411
149.520708	3660.250511	6.538406	-0.030447	3.307846
149.837085	3668.301609	6.543411	-0.030512	3.311293
150.170727	3676.334077	6.548416	-0.030579	3.314730
150.369447	3684.329037	6.553421	-0.030622	3.318142
150.785867	3692.349085	6.558426	-0.030705	3.321569
150.916514	3700.354288	6.563430	-0.030735	3.324975
151.070961	3708.389962	6.568435	-0.030769	3.328392
151.230784	3716.450446	6.573440	-0.030804	3.331816
151.587503	3724.472574	6.578445	-0.030876	3.335227
151.598324	3732.521496	6.583450	-0.030883	3.338633
151.644933	3740.547453	6.588454	-0.030898	3.342028
151.919820	3748.555092	6.593459	-0.030954	3.345420
152.102396	3756.604181	6.598464	-0.030994	3.348822
152.480491	3764.623131	6.603469	-0.031070	3.352215
152.849690	3772.676389	6.608474	-0.031144	3.355619
152.765656	3780.677544	6.613478	-0.031134	3.358981
153.010466	3788.723089	6.618483	-0.031185	3.362371
153.151404	3796.759739	6.623488	-0.031216	3.365749
153.262978	3804.754161	6.628493	-0.031243	3.369105
153.695011	3812.826935	6.633498	-0.031329	3.372502
153.899526	3820.854294	6.638502	-0.031372	3.375869
154.082421	3828.864710	6.643507	-0.031412	3.379224
154.383957	3836.889574	6.648512	-0.031473	3.382586
154.356507	3844.925703	6.653517	-0.031474	3.385938
154.698218	3852.939374	6.658522	-0.031543	3.389290
155.074694	3861.020486	6.663526	-0.031618	3.392668
155.337771	3869.090080	6.668531	-0.031673	3.396034
155.124006	3877.067977	6.673536	-0.031638	3.399341
155.358277	3885.040906	6.678541	-0.031687	3.402659
155.513054	3893.072051	6.683546	-0.031722	3.405996
155.669220	3901.058263	6.688550	-0.031756	3.409310
155.652655	3909.165529	6.693555	-0.031759	3.412665
155.966494	3917.163507	6.698560	-0.031822	3.415983
156.130135	3925.158393	6.703565	-0.031858	3.419292
156.524341	3933.170094	6.708570	-0.031937	3.422612
156.497368	3941.208512	6.713574	-0.031938	3.425925
156.828935	3949.223760	6.718579	-0.032005	3.429238
157.052728	3957.263337	6.723584	-0.032052	3.432554
157.080463	3965.352651	6.728589	-0.032063	3.435880
157.302182	3973.337428	6.733594	-0.032109	3.439167
157.633036	3981.331739	6.738598	-0.032176	3.442458
158.010156	3989.356018	6.743603	-0.032252	3.445760
158.247808	3997.362088	6.748608	-0.032302	3.449047
157.991891	4005.463090	6.753613	-0.032260	3.452352
158.465480	4013.493131	6.758618	-0.032353	3.455650
158.749563	4021.470567	6.763622	-0.032412	3.458917
158.981353	4029.493564	6.768627	-0.032460	3.462198
159.075973	4037.541383	6.773632	-0.032483	3.465481
159.249941	4045.579818	6.778637	-0.032521	3.468759
159.566156	4053.658398	6.783642	-0.032586	3.472056
159.655106	4061.664468	6.788646	-0.032608	3.475313
159.947183	4069.667401	6.793651	-0.032667	3.478571
160.089739	4077.702110	6.798656	-0.032700	3.481835
160.249467	4085.647505	6.803661	-0.032735	3.485060
160.510016	4093.728197	6.808666	-0.032789	3.488340
160.524342	4101.752525	6.813670	-0.032797	3.491586
160.636642	4109.778994	6.818675	-0.032823	3.494833
160.861547	4117.796468	6.823680	-0.032871	3.498078
161.086656	4125.781988	6.828685	-0.032918	3.501306
161.414324	4133.807333	6.833690	-0.032984	3.504550
161.440338	4141.852765	6.838694	-0.032995	3.507790
161.922775	4149.892154	6.843699	-0.033090	3.511039
162.427885	4157.932034	6.848704	-0.033189	3.514285
162.365311	4165.954739	6.853709	-0.033183	3.517505
162.436206	4174.018151	6.858714	-0.033202	3.520741
162.501693	4181.991232	6.863718	-0.033220	3.523938
162.849283	4189.994549	6.868723	-0.033290	3.527153
162.942426	4198.048891	6.873728	-0.033313	3.530378
163.091478	4206.087650	6.878733	-0.033346	3.533595
163.377035	4214.138347	6.883738	-0.033404	3.536818
163.414393	4222.146354	6.888742	-0.033417	3.540014
163.546281	4230.149021	6.893747	-0.033447	3.543208
163.705935	4238.216505	6.898752	-0.033482	3.546425
163.918782	4246.213612	6.903757	-0.033527	3.549613
164.068389	4254.359470	6.908762	-0.033561	3.552855
164.259306	4262.387067	6.913766	-0.033602	3.556048
164.370558	4270.334998	6.918771	-0.033628	3.559205
164.539005	4278.341749	6.923776	-0.033665	3.562384
164.720033	4286.324049	6.928781	-0.033704	3.565551
164.926277	4294.359037	6.933786	-0.033748	3.568736
164.964842	4302.370179	6.938790	-0.033760	3.571904
165.378450	4310.407615	6.943795	-0.033843	3.575091
165.888893	4318.435840	6.948800	-0.033943	3.578274
165.749716	4326.454663	6.953805	-0.033923	3.581431
165.903783	4334.478999	6.958810	-0.033957	3.584597
166.320580	4342.481130	6.963814	-0.034040	3.587758
166.799325	4350.516218	6.968819	-0.034135	3.590931
166.870789	4358.555428	6.973824	-0.034153	3.594092
167.043494	4366.561845	6.978829	-0.034191	3.597239
167.234523	4374.598734	6.983834	-0.034232	3.600397
167.243838	4382.580050	6.988838	-0.034239	3.603524
167.506485	4390.634001	6.993843	-0.034294	3.606685
167.968451	4398.620268	6.998848	-0.034385	3.609821
167.900392	4406.705668	7.003853	-0.034378	3.612979
168.127159	4414.767649	7.008858	-0.034426	3.616133
168.537772	4422.672483	7.013862	-0.034507	3.619228
168.717038	4430.739189	7.018867	-0.034546	3.622378
168.886456	4438.775198	7.023872	-0.034583	3.625512
168.960644	4446.796014	7.028877	-0.034603	3.628635
169.393916	4454.851737	7.033882	-0.034689	3.631778
169.400958	4462.887224	7.038886	-0.034695	3.634900
169.336659	4470.920095	7.043891	-0.034689	3.638015
169.771222	4478.939795	7.048896	-0.034775	3.641137
169.859423	4486.879235	7.053901	-0.034797	3.644215
169.949106	4494.952820	7.058906	-0.034819	3.647343
169.959626	4502.986324	7.063910	-0.034827	3.650450
170.312539	4511.044470	7.068915	-0.034898	3.653573
170.378432	4519.084775	7.073920	-0.034916	3.656679
170.459035	4527.035415	7.078925	-0.034936	3.659749
170.692987	4535.065828	7.083930	-0.034985	3.662850
170.772908	4543.110339	7.088934	-0.035006	3.665950
170.964352	4551.144438	7.093939	-0.035047	3.669047
171.317432	4559.181040	7.098944	-0.035118	3.672145
171.356025	4567.199349	7.103949	-0.035130	3.675227
171.647839	4575.217237	7.108954	-0.035190	3.678311
171.729515	4583.235649	7.113958	-0.035211	3.681388
172.173310	4591.200048	7.118963	-0.035299	3.684451
172.177091	4599.254302	7.123968	-0.035305	3.687535
172.390917	4607.278558	7.128973	-0.035350	3.690610
172.795840	4615.327247	7.133978	-0.035431	3.693696
172.777661	4623.334602	7.138982	-0.035433	3.696754
172.924491	4631.353325	7.143987	-0.035466	3.699817
173.230181	4639.355278	7.148992	-0.035529	3.702875
173.411525	4647.367170	7.153997	-0.035568	3.705932
173.658633	4655.403651	7.159002	-0.035619	3.708997
173.777444	4663.489697	7.164006	-0.035647	3.712075
174.002501	4671.538668	7.169011	-0.035694	3.715139
174.113166	4679.519488	7.174016	-0.035720	3.718171
174.203769	4687.509813	7.179021	-0.035743	3.721205
174.229331	4695.505098	7.184026	-0.035753	3.724236
174.361380	4703.521566	7.189030	-0.035783	3.727275
174.681764	4711.558254	7.194035	-0.035848	3.730324
175.141135	4719.589551	7.199040	-0.035939	3.733372
174.928106	4727.637873	7.204045	-0.035905	3.736407
175.085070	4735.669343	7.209050	-0.035940	3.739443
175.392080	4743.638371	7.214054	-0.036002	3.742456
175.561430	4751.693855	7.219059	-0.036039	3.745496
175.755934	4759.707118	7.224064	-0.036081	3.748518
175.898368	4767.731842	7.229069	-0.036113	3.751540
176.203083	4775.795411	7.234074	-0.036175	3.754579
176.339265	4783.791268	7.239078	-0.036206	3.757586
176.389342	4791.810554	7.244083	-0.036221	3.760597
176.560562	4799.822191	7.249088	-0.036258	3.763606
176.755753	4807.848855	7.254093	-0.036300	3.766618
176.901788	4815.877532	7.259098	-0.036332	3.769628
176.995622	4823.929230	7.264102	-0.036355	3.772642
177.266743	4831.942409	7.269107	-0.036411	3.775644
177.455442	4839.963730	7.274112	-0.036452	3.778645
177.557614	4847.998407	7.279117	-0.036476	3.781646
177.784765	4855.984275	7.284122	-0.036524	3.784629
177.708235	4864.038319	7.289126	-0.036515	3.787629
178.110866	4872.019793	7.294131	-0.036596	3.790610
178.257052	4880.136318	7.299136	-0.036628	3.793633
178.378197	4888.102089	7.304141	-0.036656	3.796597
178.581706	4896.083569	7.309146	-0.036700	3.799566
178.839155	4904.103553	7.314150	-0.036753	3.802549
179.004195	4912.125274	7.319155	-0.036789	3.805527
179.107375	4920.137595	7.324160	-0.036814	3.808499
179.343059	4928.167054	7.329165	-0.036863	3.811477
179.772096	4936.182377	7.334170	-0.036949	3.814452
179.694205	4944.198888	7.339174	-0.036940	3.817414
179.834055	4952.205644	7.344179	-0.036971	3.820375
180.072650	4960.241765	7.349184	-0.037021	3.823347
180.234214	4968.238708	7.354189	-0.037057	3.826300
180.562196	4976.252731	7.359194	-0.037123	3.829261
180.602787	4984.295416	7.364198	-0.037136	3.832223
180.764481	4992.345112	7.369203	-0.037172	3.835189
181.048919	5000.355951	7.374208	-0.037230	3.838140
180.979837	5008.393019	7.379213	-0.037223	3.841092
181.517611	5016.370672	7.384218	-0.037328	3.844032
181.437877	5024.412236	7.389222	-0.037319	3.846980
181.913269	5032.405963	7.394227	-0.037413	3.849920
182.294871	5040.478591	7.399232	-0.037489	3.852885
182.462062	5048.499515	7.404237	-0.037526	3.855824
182.622654	5056.523587	7.409242	-0.037561	3.858762
182.764985	5064.529217	7.414246	-0.037593	3.861690
183.073400	5072.523334	7.419251	-0.037656	3.864616
183.273318	5080.595484	7.424256	-0.037699	3.867565
183.285364	5088.638716	7.429261	-0.037707	3.870498
183.575012	5096.878752	7.434266	-0.037766	3.873506
183.975978	5104.837907	7.439270	-0.037846	3.876411
183.854561	5112.748916	7.444275	-0.037829	3.879286
183.913886	5120.749707	7.449280	-0.037846	3.882196
184.106259	5128.716746	7.454285	-0.037887	3.885093
184.272750	5136.735947	7.459290	-0.037923	3.888007
184.327080	5144.771502	7.464294	-0.037939	3.890922
184.600855	5152.793755	7.469299	-0.037995	3.893835
184.905916	5160.814454	7.474304	-0.038058	3.896745
185.055784	5168.803688	7.479309	-0.038091	3.899639
185.098568	5176.852035	7.484314	-0.038104	3.902550
185.367537	5184.817701	7.489318	-0.038160	3.905433
185.573092	5192.843705	7.494323	-0.038204	3.908335
185.919444	5200.893595	7.499328	-0.038274	3.911245
186.038186	5208.894653	7.504333	-0.038301	3.914132
186.188052	5216.959034	7.509338	-0.038334	3.917040
186.495235	5224.919924	7.514342	-0.038397	3.919911
186.524201	5232.941767	7.519347	-0.038408	3.922797
186.688009	5240.993978	7.524352	-0.038444	3.925694
186.644340	5248.989657	7.529357	-0.038441	3.928565
186.885039	5257.056917	7.534362	-0.038492	3.931465
187.046777	5265.056697	7.539366	-0.038527	3.934337
187.307918	5273.058305	7.544371	-0.038581	3.937209
187.532436	5281.066826	7.549376	-0.038628	3.940081
187.593900	5289.058827	7.554381	-0.038645	3.942942
187.892828	5297.140145	7.559386	-0.038706	3.945837
187.983677	5305.138997	7.564390	-0.038729	3.948697
188.260117	5313.166967	7.569395	-0.038786	3.951568
188.472758	5321.215394	7.574400	-0.038831	3.954444
188.558455	5329.219007	7.579405	-0.038852	3.957299
188.717344	5337.217013	7.584410	-0.038887	3.960151
188.701285	5345.213502	7.589414	-0.038890	3.962997
189.074622	5353.255865	7.594419	-0.038965	3.965865
188.998858	5361.293183	7.599424	-0.038956	3.968721
189.141694	5369.270470	7.604429	-0.038988	3.971557
189.481069	5377.348901	7.609434	-0.039057	3.974431
189.492644	5385.369575	7.614438	-0.039064	3.977276
189.709983	5393.351966	7.619443	-0.039110	3.980110
190.118100	5401.378818	7.624448	-0.039192	3.982960
190.254373	5409.408400	7.629453	-0.039223	3.985804
190.145265	5417.455180	7.634458	-0.039208	3.988648
190.331643	5425.477211	7.639462	-0.039248	3.991487
190.624199	5433.508105	7.644467	-0.039308	3.994328
190.806441	5441.521594	7.649472	-0.039347	3.997160
190.697576	5449.502786	7.654477	-0.039332	3.999973
191.132022	5457.544600	7.659482	-0.039419	4.002814
191.150513	5465.546423	7.664486	-0.039428	4.005633
191.132831	5473.568838	7.669491	-0.039430	4.008456
191.660559	5481.621265	7.674496	-0.039534	4.011296
191.837928	5489.616201	7.679501	-0.039572	4.014109
191.960116	5497.665524	7.684506	-0.039600	4.016938
192.118004	5505.661156	7.689510	-0.039635	4.019746
192.452027	5513.670713	7.694515	-0.039703	4.022561
192.509695	5521.703512	7.699520	-0.039719	4.025377
192.474548	5529.719272	7.704525	-0.039718	4.028183
192.850473	5537.770912	7.709530	-0.039793	4.031007
192.802236	5545.862819	7.714534	-0.039790	4.033836
192.975264	5553.851653	7.719539	-0.039828	4.036631
193.263493	5561.793758	7.724544	-0.039887	4.039409
193.167021	5569.823234	7.729549	-0.039874	4.042209
193.482797	5577.832641	7.734554	-0.039938	4.045007
193.634621	5585.820625	7.739558	-0.039972	4.047793
193.843947	5593.839560	7.744563	-0.040017	4.050589
194.009536	5601.925194	7.749568	-0.040053	4.053405
194.238672	5609.920479	7.754573	-0.040101	4.056189
194.523709	5617.891178	7.759578	-0.040159	4.058963
194.531200	5625.948188	7.764582	-0.040166	4.061762
194.572836	5633.913071	7.769587	-0.040180	4.064527
194.995560	5641.992046	7.774592	-0.040264	4.067335
194.925316	5649.941911	7.779597	-0.040256	4.070089
195.021815	5658.058993	7.784602	-0.040280	4.072901
195.177713	5666.065635	7.789606	-0.040314	4.075675
195.283269	5674.042806	7.794611	-0.040339	4.078435
195.514552	5682.064677	7.799616	-0.040388	4.081211
195.417481	5690.051844	7.804621	-0.040375	4.083968
195.773845	5698.100598	7.809626	-0.040447	4.086751
195.809848	5706.087952	7.814630	-0.040459	4.089507
195.910079	5714.130747	7.819635	-0.040483	4.092280
196.205577	5722.177768	7.824640	-0.040544	4.095056
196.438090	5730.173852	7.829645	-0.040592	4.097812
196.300501	5738.187918	7.834650	-0.040572	4.100566
196.587690	5746.180079	7.839654	-0.040631	4.103317
196.717056	5754.248321	7.844659	-0.040661	4.106091
196.814173	5762.282369	7.849664	-0.040684	4.108850
196.900032	5770.295891	7.854669	-0.040706	4.111600
197.247763	5778.352322	7.859674	-0.040776	4.114367
197.623240	5786.322127	7.864678	-0.040851	4.117102
197.572879	5794.332436	7.869683	-0.040847	4.119843
197.735085	5802.366652	7.874688	-0.040883	4.122594
197.872472	5810.317708	7.879693	-0.040914	4.125314
198.218876	5818.371517	7.884698	-0.040984	4.128071
198.357332	5826.406442	7.889702	-0.041015	4.130816
198.531199	5834.436338	7.894707	-0.041053	4.133558
198.631206	5842.505456	7.899712	-0.041077	4.136310
198.526991	5850.471858	7.904717	-0.041063	4.139024
198.875234	5858.539165	7.909722	-0.041134	4.141775
199.073649	5866.509024	7.914726	-0.041176	4.144490
199.378296	5874.569521	7.919731	-0.041238	4.147235
199.409123	5882.583550	7.924736	-0.041249	4.149959
199.501036	5890.630154	7.929741	-0.041272	4.152693
199.678884	5898.675439	7.934746	-0.041311	4.155425
199.726422	5906.615510	7.939750	-0.041325	4.158119
200.126679	5914.642609	7.944755	-0.041405	4.160844
200.400624	5922.657335	7.949760	-0.041461	4.163562
200.365923	5930.665768	7.954765	-0.041460	4.166273
200.506472	5938.693798	7.959770	-0.041492	4.168990
200.629324	5946.748049	7.964774	-0.041520	4.171715
200.655543	5954.716563	7.969779	-0.041531	4.174407
200.881087	5962.765020	7.974784	-0.041578	4.177127
201.022463	5970.743851	7.979789	-0.041610	4.179821
201.294490	5978.805113	7.984794	-0.041666	4.182542
201.534458	5986.789376	7.989798	-0.041716	4.185235
201.756029	5994.820292	7.994803	-0.041763	4.187942
201.850272	6002.852256	7.999808	-0.041786	4.190646
201.710393	6010.955460	8.004813	-0.041765	4.193369
202.031299	6018.996240	8.009818	-0.041830	4.196075
202.104641	6026.892116	8.014822	-0.041849	4.198728
202.219283	6034.911747	8.019827	-0.041876	4.201421
202.415058	6042.872593	8.024832	-0.041918	4.204093
202.405562	6050.910186	8.029837	-0.041922	4.206788
202.869211	6058.909425	8.034842	-0.042014	4.209472
202.853620	6066.929607	8.039846	-0.042016	4.212157
202.996576	6074.936072	8.044851	-0.042048	4.214837
203.224436	6082.959137	8.049856	-0.042096	4.217522
203.370631	6090.990810	8.054861	-0.042129	4.220207
203.545561	6099.009036	8.059866	-0.042167	4.222887
203.621232	6107.010117	8.064870	-0.042186	4.225558
203.738369	6115.058150	8.069875	-0.042214	4.228243
203.937926	6123.083638	8.074880	-0.042256	4.230920
203.993074	6131.125068	8.079885	-0.042272	4.233599
204.206789	6139.162343	8.084890	-0.042317	4.236276
204.260632	6147.127717	8.089894	-0.042333	4.238926
204.399858	6155.129487	8.094899	-0.042364	4.241588
204.587758	6163.117107	8.099904	-0.042405	4.244243
204.871646	6171.157902	8.104909	-0.042463	4.246916
205.011972	6179.190018	8.109914	-0.042494	4.249582
205.008106	6187.213354	8.114918	-0.042499	4.252243
205.092548	6195.268499	8.119923	-0.042520	4.254913
205.216304	6203.311641	8.124928	-0.042549	4.257578
205.493322	6211.271738	8.129933	-0.042606	4.260215
205.688336	6219.292917	8.134938	-0.042648	4.262870
205.708328	6227.281360	8.139942	-0.042657	4.265511
205.802285	6235.327631	8.144947	-0.042680	4.268170
206.138600	6243.404727	8.149952	-0.042748	4.270840
205.979471	6251.409143	8.154957	-0.042724	4.273479
206.309868	6259.485272	8.159962	-0.042791	4.276145
206.512263	6267.441002	8.164966	-0.042834	4.278769
206.387560	6275.482156	8.169971	-0.042816	4.281416
206.599310	6283.437136	8.174976	-0.042861	4.284036
206.640162	6291.468803	8.179981	-0.042874	4.286678
206.923567	6299.460424	8.184986	-0.042932	4.289307
207.111348	6307.542152	8.189990	-0.042973	4.291964
207.248830	6315.585504	8.194995	-0.043004	4.294606
207.430837	6323.572820	8.200000	-0.043043	4.297228
207.471689	6331.544710	8.205005	-0.043056	4.299842
207.711877	6339.563374	8.210010	-0.043106	4.302472
207.926797	6347.578117	8.215014	-0.043152	4.305098
208.028410	6355.592899	8.220019	-0.043176	4.307722
208.124114	6363.641398	8.225024	-0.043200	4.310356
208.302862	6371.676691	8.230029	-0.043238	4.312984
208.301726	6379.713473	8.235034	-0.043244	4.315610
208.463969	6387.666287	8.240038	-0.043279	4.318207
208.497099	6395.703461	8.245043	-0.043291	4.320830
208.773071	6403.693147	8.250048	-0.043348	4.323438
208.984320	6411.723717	8.255053	-0.043392	4.326056
209.328558	6419.722745	8.260058	-0.043462	4.328664
209.615731	6427.760614	8.265062	-0.043521	4.331283
209.700293	6435.811715	8.270067	-0.043542	4.333902
209.921297	6443.839816	8.275072	-0.043589	4.336514
209.778375	6451.772009	8.280077	-0.043568	4.339090
210.084775	6459.870553	8.285082	-0.043630	4.341722
210.292949	6467.806831	8.290086	-0.043674	4.344299
210.198311	6475.873599	8.295091	-0.043662	4.346915
210.559063	6483.892474	8.300096	-0.043735	4.349516
210.676947	6491.928962	8.305101	-0.043762	4.352120
210.924759	6499.955158	8.310106	-0.043814	4.354720
210.834458	6507.980465	8.315110	-0.043802	4.357316
211.170110	6515.932564	8.320115	-0.043870	4.359890
211.297977	6523.961221	8.325120	-0.043900	4.362485
211.324083	6531.931906	8.330125	-0.043910	4.365059
211.564367	6540.005761	8.335130	-0.043960	4.367667
211.505404	6548.014720	8.340134	-0.043955	4.370250
211.691501	6556.038322	8.345139	-0.043995	4.372838
212.043039	6564.085003	8.350144	-0.044066	4.375432
212.087897	6572.042366	8.355149	-0.044079	4.377995
212.098506	6580.054532	8.360154	-0.044087	4.380573
212.306074	6588.081472	8.365158	-0.044131	4.383156
212.618744	6596.110392	8.370163	-0.044195	4.385739
212.606282	6604.142138	8.375168	-0.044198	4.388319
212.502541	6612.115034	8.380173	-0.044184	4.390878
212.729845	6620.191950	8.385178	-0.044232	4.393471
212.804302	6628.203304	8.390182	-0.044251	4.396040
212.893865	6636.157739	8.395187	-0.044273	4.398590
213.147296	6644.225251	8.400192	-0.044326	4.401175
213.238346	6652.158832	8.405197	-0.044348	4.403715
213.396767	6660.230650	8.410202	-0.044383	4.406298
213.495967	6668.253531	8.415206	-0.044407	4.408864
213.759846	6676.255061	8.420211	-0.044462	4.411422
214.006242	6684.333986	8.425216	-0.044513	4.414004
214.058811	6692.333670	8.430221	-0.044528	4.416557
214.157045	6700.333397	8.435226	-0.044552	4.419109
214.315430	6708.392723	8.440230	-0.044587	4.421679
214.264536	6716.334471	8.445235	-0.044583	4.424209
214.500813	6724.445210	8.450240	-0.044632	4.426793
214.776156	6732.419894	8.455245	-0.044689	4.429332
214.835674	6740.470116	8.460250	-0.044706	4.431893
214.903349	6748.495437	8.465254	-0.044724	4.434444
215.127168	6756.482932	8.470259	-0.044771	4.436983
215.397172	6764.478397	8.475264	-0.044827	4.439523
215.421352	6772.505510	8.480269	-0.044837	4.442070
215.594288	6780.464359	8.485274	-0.044874	4.444595
215.627764	6788.530147	8.490278	-0.044886	4.447151
215.684286	6796.523401	8.495283	-0.044902	4.449683
215.813691	6804.614019	8.500288	-0.044931	4.452245
215.967517	6812.568895	8.505293	-0.044966	4.454763
216.236683	6820.616778	8.510298	-0.045021	4.457309
216.378488	6828.615595	8.515302	-0.045053	4.459837
216.515319	6836.613144	8.520307	-0.045084	4.462364
216.633646	6844.635292	8.525312	-0.045111	4.464897
216.763542	6852.653007	8.530317	-0.045141	4.467427
216.814785	6860.709899	8.535322	-0.045156	4.469968
216.913389	6868.746097	8.540326	-0.045180	4.472501
217.065644	6876.745654	8.545331	-0.045214	4.475021
217.182204	6884.756128	8.550336	-0.045241	4.477543
217.396389	6892.696678	8.555341	-0.045286	4.480041
217.604070	6900.721277	8.560346	-0.045330	4.482565
217.605678	6908.737696	8.565351	-0.045336	4.485084
217.866068	6916.792817	8.570355	-0.045390	4.487615
218.149214	6924.783724	8.575360	-0.045448	4.490124
218.043019	6932.836741	8.580365	-0.045434	4.492650
218.260172	6940.842388	8.585370	-0.045480	4.495161
218.527038	6948.851146	8.590375	-0.045535	4.497671
218.695710	6956.838461	8.595379	-0.045572	4.500173
218.891281	6964.894907	8.600384	-0.045614	4.502696
218.915974	6972.857616	8.605389	-0.045624	4.505187
219.002411	6980.934095	8.610394	-0.045645	4.507712
219.177594	6988.947449	8.615399	-0.045683	4.510217
219.129794	6996.978143	8.620403	-0.045680	4.512724
219.326326	7005.044376	8.625408	-0.045722	4.515243
219.583699	7013.003609	8.630413	-0.045775	4.517726
219.779690	7020.984821	8.635418	-0.045817	4.520215
219.942296	7028.983790	8.640423	-0.045853	4.522708
220.120919	7036.957048	8.645427	-0.045892	4.525192
220.159459	7045.028039	8.650432	-0.045904	4.527704
220.291697	7053.020589	8.655437	-0.045934	4.530190
220.430436	7061.086852	8.660442	-0.045966	4.532699
220.370880	7069.085544	8.665447	-0.045960	4.535184
220.320758	7077.098607	8.670451	-0.045956	4.537673
220.765468	7085.112094	8.675456	-0.046044	4.540161
220.829171	7093.112229	8.680461	-0.046062	4.542643
220.777149	7101.136556	8.685466	-0.046058	4.545131
220.982258	7109.117525	8.690471	-0.046101	4.547604
221.222550	7117.128961	8.695475	-0.046151	4.550086
221.418737	7125.249005	8.700480	-0.046193	4.552600
221.442669	7133.242218	8.705485	-0.046203	4.555073
221.588470	7141.244280	8.710490	-0.046236	4.557547
221.718305	7149.234659	8.715495	-0.046266	4.560017
221.814632	7157.270012	8.720499	-0.046289	4.562499
222.295095	7165.308239	8.725504	-0.046384	4.564981
222.373417	7173.308043	8.730509	-0.046404	4.567449
222.509679	7181.310990	8.735514	-0.046435	4.569917
222.539559	7189.356182	8.740519	-0.046446	4.572397
222.653643	7197.355809	8.745523	-0.046472	4.574861
222.812111	7205.406328	8.750528	-0.046507	4.577339
222.920255	7213.299036	8.755533	-0.046533	4.579768
222.878224	7221.410649	8.760538	-0.046531	4.582262
222.991431	7229.368805	8.765543	-0.046557	4.584708
223.144622	7237.460278	8.770547	-0.046591	4.587194
223.426348	7245.467451	8.775552	-0.046649	4.589653
223.368514	7253.490870	8.780557	-0.046644	4.592115
223.717255	7261.550476	8.785562	-0.046714	4.594587
223.942887	7269.558719	8.790567	-0.046762	4.597042
223.797188	7277.498429	8.795571	-0.046740	4.599474
224.156166	7285.575339	8.800576	-0.046812	4.601947
224.029197	7293.515346	8.805581	-0.046794	4.604377
224.364400	7301.595984	8.810586	-0.046862	4.606849
224.497207	7309.545343	8.815591	-0.046892	4.609279
224.545253	7317.617546	8.820595	-0.046907	4.611745
224.849146	7325.638841	8.825600	-0.046969	4.614195
224.920988	7333.633816	8.830605	-0.046987	4.616635
224.885263	7341.627912	8.835610	-0.046986	4.619074
225.007688	7349.714383	8.840615	-0.047014	4.621539
225.200624	7357.610560	8.845619	-0.047056	4.623945
225.309358	7365.679019	8.850624	-0.047082	4.626402
225.350304	7373.668651	8.855629	-0.047095	4.628835
225.588136	7381.746919	8.860634	-0.047144	4.631292
225.602573	7389.765588	8.865639	-0.047153	4.633730
225.631902	7397.788518	8.870643	-0.047163	4.636169
226.068527	7405.739323	8.875648	-0.047250	4.638584
226.047218	7413.738790	8.880653	-0.047252	4.641012
226.078302	7421.799166	8.885658	-0.047263	4.643458
226.290086	7429.811730	8.890663	-0.047308	4.645888
226.484919	7437.787325	8.895667	-0.047349	4.648305
226.661318	7445.842352	8.900672	-0.047388	4.650745
226.709031	7453.867269	8.905677	-0.047402	4.653175
227.084342	7461.918084	8.910682	-0.047478	4.655611
227.116516	7469.914299	8.915687	-0.047489	4.658030
227.109207	7477.836045	8.920691	-0.047493	4.660425
227.448471	7485.908896	8.925696	-0.047562	4.662864
227.603887	7493.940923	8.930701	-0.047596	4.665289
227.800220	7501.944261	8.935706	-0.047638	4.667705
227.717791	7509.973391	8.940711	-0.047628	4.670127
227.739644	7518.058924	8.945715	-0.047638	4.672565
228.087219	7526.107753	8.950720	-0.047708	4.674990
228.040434	7534.005522	8.955725	-0.047705	4.677369
228.278120	7542.028046	8.960730	-0.047754	4.679784
228.170705	7550.047790	8.965735	-0.047740	4.682197
228.446370	7557.967836	8.970739	-0.047797	4.684579
228.728918	7566.069718	8.975744	-0.047855	4.687014
228.637208	7574.063541	8.980749	-0.047843	4.689415
228.871471	7582.120621	8.985754	-0.047892	4.691834
229.061145	7590.125489	8.990759	-0.047933	4.694236
229.150425	7598.130765	8.995763	-0.047955	4.696638
229.416499	7606.096572	9.000768	-0.048010	4.699025
229.377650	7614.137395	9.005773	-0.048008	4.701435
229.558659	7622.140098	9.010778	-0.048047	4.703831
229.591633	7630.177182	9.015783	-0.048059	4.706237
229.614849	7638.120215	9.020787	-0.048069	4.708614
229.796521	7646.203201	9.025792	-0.048108	4.711030
229.758551	7654.239587	9.030797	-0.048106	4.713432
229.854523	7662.279052	9.035802	-0.048130	4.715834
230.128313	7670.270785	9.040807	-0.048186	4.718219
230.386988	7678.262363	9.045811	-0.048240	4.720604
230.534633	7686.306338	9.050816	-0.048273	4.723003
230.373482	7694.252235	9.055821	-0.048248	4.725372
230.533091	7702.328621	9.060826	-0.048283	4.727778
230.752240	7710.392964	9.065831	-0.048330	4.730179
230.955339	7718.394204	9.070835	-0.048373	4.732560
230.986225	7726.444092	9.075840	-0.048384	4.734955
231.117188	7734.374087	9.080845	-0.048414	4.737313
231.061447	7742.435460	9.085850	-0.048409	4.739709
231.121658	7750.460031	9.090855	-0.048426	4.742093
231.408658	7758.375332	9.095859	-0.048485	4.744442
231.646138	7766.501449	9.100864	-0.048534	4.746853
231.539464	7774.421742	9.105869	-0.048520	4.749202
231.883659	7782.500437	9.110874	-0.048589	4.751596
232.297351	7790.573585	9.115879	-0.048672	4.753987
232.498723	7798.582128	9.120883	-0.048715	4.756358
232.528637	7806.580113	9.125888	-0.048726	4.758726
232.491585	7814.511654	9.130893	-0.048724	4.761073
232.776061	7822.549146	9.135898	-0.048783	4.763448
232.759967	7830.533240	9.140903	-0.048785	4.765808
232.791082	7838.525047	9.145907	-0.048796	4.768169
232.993331	7846.597007	9.150912	-0.048840	4.770552
233.062887	7854.601567	9.155917	-0.048858	4.772914
233.281514	7862.672394	9.160922	-0.048904	4.775294
233.334967	7870.659382	9.165927	-0.048920	4.777649
233.314133	7878.650412	9.170931	-0.048921	4.780003
233.579131	7886.706489	9.175936	-0.048976	4.782375
233.868794	7894.713976	9.180941	-0.049035	4.784731
234.071005	7902.692477	9.185946	-0.049078	4.787078
233.881267	7910.684329	9.190951	-0.049049	4.789429
234.171945	7918.768697	9.195955	-0.049108	4.791805
234.515702	7926.822889	9.200960	-0.049178	4.794170
234.334856	7934.796945	9.205965	-0.049149	4.796512
234.585822	7942.745077	9.210970	-0.049202	4.798844
234.859306	7950.809285	9.215975	-0.049258	4.801208
234.979174	7958.720819	9.220979	-0.049286	4.803528
235.052242	7966.851802	9.225984	-0.049305	4.805910
234.941374	7974.772911	9.230989	-0.049290	4.808231
235.306827	7982.870663	9.235994	-0.049363	4.810601
235.497207	7990.351925	9.240999	-0.049404	4.812789
235.570325	7994.860910	9.246003	-0.049421	4.814108

235.682595	7997.300716	9.251008	-0.049443	4.814821
235.729040	7998.577194	9.256013	-0.049453	4.815194
235.848266	7999.096932	9.261018	-0.049476	4.815345
235.904032	7999.775808	9.266023	-0.049487	4.815544
235.714821	7999.750335	9.271027	-0.049452	4.815537
235.813420	7999.763700	9.276032	-0.049470	4.815541
236.082552	7999.737128	9.281037	-0.049521	4.815532
236.228010	7999.828127	9.286042	-0.049548	4.815557
236.079520	7999.815059	9.291047	-0.049521	4.815554
235.936078	7999.796735	9.296051	-0.049494	4.815550
236.210237	7999.808681	9.301056	-0.049545	4.815552
236.246487	7999.791140	9.306061	-0.049552	4.815547
236.431591	7999.849686	9.311066	-0.049587	4.815563
236.597550	7999.832116	9.316071	-0.049618	4.815557
236.708842	7999.826470	9.321075	-0.049639	4.815555
236.782367	7999.795654	9.326080	-0.049653	4.815545
236.658457	7999.788323	9.331085	-0.049630	4.815544
236.872228	7999.830253	9.336090	-0.049670	4.815555
236.731170	7999.797019	9.341095	-0.049644	4.815546
236.618173	7999.800542	9.346099	-0.049623	4.815547
236.805115	7999.820682	9.351104	-0.049659	4.815552
236.897366	7999.791238	9.356109	-0.049676	4.815543
236.860816	7999.787461	9.361114	-0.049669	4.815542
236.745801	7999.805899	9.366119	-0.049648	4.815548
236.649102	7999.741356	9.371123	-0.049630	4.815530
236.794301	7999.786442	9.376128	-0.049658	4.815542
236.872415	7999.866740	9.381133	-0.049673	4.815566
237.185737	7999.827008	9.386138	-0.049731	4.815552
237.088230	7999.828647	9.391143	-0.049713	4.815553
237.031710	7999.864050	9.396147	-0.049703	4.815564
237.320995	7999.895464	9.401152	-0.049757	4.815572
237.071569	7999.880754	9.406157	-0.049711	4.815569
237.229907	7999.794728	9.411162	-0.049740	4.815543
237.074670	7999.927824	9.416167	-0.049712	4.815582
237.196894	7999.823060	9.421171	-0.049735	4.815551
237.272870	7999.840330	9.426176	-0.049749	4.815556
237.192667	7999.823032	9.431181	-0.049734	4.815551
237.382547	7999.864575	9.436186	-0.049770	4.815562
237.374775	7999.827099	9.441191	-0.049769	4.815552
237.326616	7999.921363	9.446195	-0.049760	4.815579
237.413957	7999.850198	9.451200	-0.049777	4.815558
237.375209	7999.822896	9.456205	-0.049770	4.815550
237.207154	7999.845811	9.461210	-0.049739	4.815558
237.318319	7999.831622	9.466215	-0.049759	4.815553
237.374988	7999.923318	9.471219	-0.049770	4.815580
237.370940	7999.825043	9.476224	-0.049770	4.815551
237.366304	7999.879441	9.481229	-0.049769	4.815567
237.477159	7999.819336	9.486234	-0.049790	4.815549
237.437828	7999.824056	9.491239	-0.049783	4.815550
237.294727	7999.902896	9.496243	-0.049757	4.815574
237.527023	7999.831952	9.501248	-0.049800	4.815552
237.579107	7999.818939	9.506253	-0.049810	4.815548
237.455003	7999.897020	9.511258	-0.049787	4.815572
237.392865	7999.823427	9.516263	-0.049776	4.815550
237.523203	7999.892830	9.521267	-0.049800	4.815570
237.567817	7999.873289	9.526272	-0.049809	4.815564
237.364792	7999.789933	9.531277	-0.049771	4.815541
237.544722	7999.912460	9.536282	-0.049805	4.815576
237.524195	7999.813917	9.541287	-0.049801	4.815547
237.440400	7999.894789	9.546291	-0.049786	4.815571
237.390077	7999.806440	9.551296	-0.049777	4.815545
237.586686	7999.879056	9.556301	-0.049814	4.815566
237.662961	7999.848285	9.561306	-0.049828	4.815556
237.525242	7999.864218	9.566311	-0.049803	4.815562
237.624574	7999.870124	9.571315	-0.049821	4.815563
237.703379	7999.865018	9.576320	-0.049836	4.815561
237.617342	7999.875385	9.581325	-0.049821	4.815564
237.659684	7999.808828	9.586330	-0.049829	4.815545
237.659865	7999.827002	9.591335	-0.049829	4.815550
237.469030	7999.891187	9.596339	-0.049794	4.815570
237.652308	7999.813040	9.601344	-0.049828	4.815546
237.715114	7999.895227	9.606349	-0.049840	4.815570
237.678691	7999.892520	9.611354	-0.049833	4.815569
237.574975	7999.886584	9.616359	-0.049814	4.815568
237.652013	7999.884653	9.621363	-0.049829	4.815567
238.018456	7999.803076	9.626368	-0.049897	4.815541
237.734192	7999.988530	9.631373	-0.049845	4.815597
237.792151	7999.883788	9.636378	-0.049856	4.815566
238.002240	7999.922458	9.641383	-0.049895	4.815576
237.837369	7999.843990	9.646387	-0.049864	4.815554
237.888147	7999.874732	9.651392	-0.049874	4.815563
237.981323	7999.798324	9.656397	-0.049892	4.815540
237.899493	7999.871754	9.661402	-0.049877	4.815562
237.939486	7999.907659	9.666407	-0.049884	4.815572
237.607531	7999.804055	9.671411	-0.049823	4.815543
237.817830	7999.909993	9.676416	-0.049862	4.815573
237.602010	7999.926792	9.681421	-0.049822	4.815579
237.613781	7999.837316	9.686426	-0.049825	4.815553
237.743778	7999.817027	9.691431	-0.049849	4.815547
237.663722	7999.907569	9.696435	-0.049835	4.815573
237.831356	7999.830236	9.701440	-0.049866	4.815550
237.858764	7999.899035	9.706445	-0.049871	4.815570
237.824536	7999.815217	9.711450	-0.049865	4.815546
237.775565	7999.887046	9.716455	-0.049856	4.815567
237.786838	7999.879776	9.721459	-0.049859	4.815565
238.021907	7999.794996	9.726464	-0.049903	4.815539
237.889963	7999.949827	9.731469	-0.049878	4.815585
238.060273	7999.863995	9.736474	-0.049910	4.815559
238.045900	7999.938522	9.741479	-0.049908	4.815581
238.047585	7999.975940	9.746483	-0.049908	4.815592
238.186807	7999.805252	9.751488	-0.049934	4.815541
238.056617	7999.892845	9.756493	-0.049910	4.815567
238.040563	7999.796509	9.761498	-0.049908	4.815539
238.118111	7999.910969	9.766503	-0.049922	4.815572
238.166041	7999.902159	9.771507	-0.049932	4.815569
238.246976	7999.857583	9.776512	-0.049947	4.815556
238.072933	7999.884670	9.781517	-0.049915	4.815565
238.133935	7999.891021	9.786522	-0.049926	4.815566
238.238862	7999.847902	9.791527	-0.049946	4.815553
238.078243	7999.834634	9.796531	-0.049916	4.815550
238.103917	7999.852155	9.801536	-0.049921	4.815555
238.190330	7999.926186	9.806541	-0.049938	4.815576
238.118473	7999.822536	9.811546	-0.049924	4.815546
238.159735	7999.930000	9.816551	-0.049932	4.815577
237.995870	7999.803501	9.821555	-0.049902	4.815541
237.963728	7999.827556	9.826560	-0.049896	4.815548
238.004728	7999.927541	9.831565	-0.049904	4.815577
237.999381	7999.833515	9.836570	-0.049903	4.815550
238.033075	7999.835150	9.841575	-0.049910	4.815550
238.256775	7999.959461	9.846579	-0.049952	4.815586
238.215100	7999.825337	9.851584	-0.049944	4.815547
238.161701	7999.912043	9.856589	-0.049935	4.815572
238.366786	7999.808624	9.861594	-0.049973	4.815541
238.156532	7999.934422	9.866599	-0.049934	4.815579
238.215730	7999.812616	9.871603	-0.049945	4.815543
238.325735	7999.845388	9.876608	-0.049966	4.815552
238.311860	7999.934873	9.881613	-0.049964	4.815578
238.337717	7999.825337	9.886618	-0.049969	4.815546
238.269064	7999.831715	9.891623	-0.049956	4.815548
238.299861	7999.897368	9.896627	-0.049962	4.815567
238.305221	7999.835547	9.901632	-0.049963	4.815549
238.459387	7999.886121	9.906637	-0.049992	4.815563
238.512505	7999.899818	9.911642	-0.050003	4.815567
238.420948	7999.922908	9.916647	-0.049986	4.815574
238.265687	7999.800818	9.921651	-0.049957	4.815539
238.349444	7999.863061	9.926656	-0.049973	4.815557
238.394107	7999.889433	9.931661	-0.049981	4.815564
238.189631	7999.898941	9.936666	-0.049944	4.815568
238.195870	7999.825390	9.941671	-0.049945	4.815547
238.224883	7999.899555	9.946675	-0.049951	4.815568
238.293381	7999.852641	9.951680	-0.049964	4.815554
238.086041	7999.834343	9.956685	-0.049925	4.815550
238.313297	7999.886105	9.961690	-0.049968	4.815564
238.435203	7999.909462	9.966695	-0.049991	4.815570
238.268730	7999.787190	9.971699	-0.049960	4.815535
238.477427	7999.909122	9.976704	-0.049999	4.815570
238.265612	7999.889682	9.981709	-0.049960	4.815565
238.397533	7999.896118	9.986714	-0.049985	4.815566
238.571466	7999.838105	9.991719	-0.050017	4.815548
238.442246	7999.880870	9.996723	-0.049993	4.815562
238.490378	7999.829353	10.001728	-0.050003	4.815546
238.360794	7999.826199	10.006733	-0.049979	4.815546
238.264904	7999.927163	10.011738	-0.049961	4.815576
238.549523	7999.892305	10.016743	-0.050014	4.815564
238.377089	7999.856422	10.021747	-0.049982	4.815555
238.344172	7999.884736	10.026752	-0.049977	4.815563
238.328564	7999.967785	10.031757	-0.049974	4.815587
238.425900	7999.810296	10.036762	-0.049992	4.815541
238.654570	7999.824711	10.041767	-0.050035	4.815544
238.498652	7999.942851	10.046771	-0.050006	4.815579
238.593994	7999.891034	10.051776	-0.050024	4.815564
238.505554	7999.817011	10.056781	-0.050008	4.815542
238.615485	7999.893560	10.061786	-0.050029	4.815564
238.519247	7999.832222	10.066791	-0.050011	4.815547
238.517527	7999.906956	10.071795	-0.050011	4.815569
238.710108	7999.842840	10.076800	-0.050047	4.815549
238.710517	7999.900525	10.081805	-0.050047	4.815566
238.753504	7999.949293	10.086810	-0.050056	4.815580
238.653376	7999.816353	10.091815	-0.050037	4.815542
238.574851	7999.956038	10.096819	-0.050023	4.815583
238.648289	7999.800295	10.101824	-0.050037	4.815537
238.442732	7999.991301	10.106829	-0.049999	4.815594
238.567085	7999.787270	10.111834	-0.050022	4.815533
238.421305	7999.920523	10.116839	-0.049995	4.815573
238.375941	7999.897383	10.121843	-0.049987	4.815567
238.652861	7999.823961	10.126848	-0.050039	4.815544
238.630838	7999.928262	10.131853	-0.050035	4.815574
238.633350	7999.834362	10.136858	-0.050035	4.815547
238.747113	7999.841570	10.141863	-0.050057	4.815548
238.762597	7999.896297	10.146867	-0.050060	4.815564
238.854058	7999.852960	10.151872	-0.050077	4.815551
238.630208	7999.896321	10.156877	-0.050036	4.815565
238.725303	7999.862652	10.161882	-0.050054	4.815555
238.745072	7999.845910	10.166887	-0.050058	4.815550
238.760020	7999.933728	10.171891	-0.050061	4.815575
238.686947	7999.848208	10.176896	-0.050047	4.815551
238.695256	7999.886802	10.181901	-0.050049	4.815562
238.718131	7999.918159	10.186906	-0.050054	4.815571
238.513617	7999.818758	10.191911	-0.050016	4.815543
238.591049	7999.876627	10.196915	-0.050030	4.815559
238.486839	7999.817295	10.201920	-0.050011	4.815542
238.517345	7999.898959	10.206925	-0.050017	4.815566
238.616661	7999.819446	10.211930	-0.050036	4.815542
238.655464	7999.933278	10.216935	-0.050043	4.815576
238.583652	7999.809341	10.221939	-0.050030	4.815540
238.557924	7999.834568	10.226944	-0.050026	4.815547
238.679262	7999.923049	10.231949	-0.050049	4.815572
239.066399	7999.811912	10.236954	-0.050121	4.815538
238.953511	7999.896585	10.241959	-0.050100	4.815563
238.876999	7999.962629	10.246963	-0.050086	4.815583
238.907459	7999.810457	10.251968	-0.050092	4.815538
238.779328	7999.901287	10.256973	-0.050068	4.815566
238.782615	7999.877870	10.261978	-0.050069	4.815559
238.887628	7999.922308	10.266983	-0.050089	4.815571
238.778744	7999.798835	10.271987	-0.050069	4.815536
238.891680	7999.914941	10.276992	-0.050090	4.815569
238.805770	7999.896480	10.281997	-0.050074	4.815564
238.900918	7999.870286	10.287002	-0.050092	4.815556
238.638416	7999.878851	10.292007	-0.050044	4.815560
238.969002	7999.846876	10.297011	-0.050105	4.815549
239.000006	7999.913601	10.302016	-0.050111	4.815568
238.935885	7999.912578	10.307021	-0.050100	4.815568
239.043117	7999.832126	10.312026	-0.050120	4.815544
239.180588	7999.862143	10.317031	-0.050146	4.815552
239.016878	7999.923566	10.322035	-0.050116	4.815571
239.020071	7999.889470	10.327040	-0.050116	4.815561
239.050842	7999.850484	10.332045	-0.050122	4.815549
239.120998	7999.823884	10.337050	-0.050136	4.815541
239.072715	7999.908539	10.342055	-0.050127	4.815566
238.823768	7999.869275	10.347059	-0.050081	4.815556
239.016188	7999.836121	10.352064	-0.050117	4.815545
238.940234	7999.900039	10.357069	-0.050103	4.815564
238.993811	7999.857153	10.362074	-0.050113	4.815552
239.004007	7999.925675	10.367079	-0.050115	4.815572
239.112967	7999.792931	10.372083	-0.050136	4.815532
238.819999	7999.905639	10.377088	-0.050081	4.815567
238.931688	7999.913882	10.382093	-0.050102	4.815568
238.925761	7999.858283	10.387098	-0.050102	4.815552
238.995700	7999.886135	10.392103	-0.050115	4.815560
239.062354	7999.812496	10.397107	-0.050127	4.815538
238.962335	7999.842923	10.402112	-0.050109	4.815547
239.070489	7999.918377	10.407117	-0.050129	4.815569
238.880270	7999.806393	10.412122	-0.050094	4.815537
239.028490	7999.924141	10.417127	-0.050122	4.815571
238.967669	7999.878326	10.422131	-0.050111	4.815558
238.918416	7999.820955	10.427136	-0.050102	4.815541
238.984456	7999.899995	10.432141	-0.050115	4.815564
239.229510	7999.829258	10.437146	-0.050160	4.815542
239.037672	7999.962831	10.442151	-0.050125	4.815582
238.721750	7999.792213	10.447155	-0.050066	4.815534
239.113159	7999.942744	10.452160	-0.050140	4.815576
239.048921	7999.825335	10.457165	-0.050128	4.815542
238.793511	7999.851099	10.462170	-0.050080	4.815551
239.129104	7999.848034	10.467175	-0.050143	4.815548
239.239540	7999.855189	10.472179	-0.050164	4.815550
239.198084	7999.950634	10.477184	-0.050157	4.815578
238.972645	7999.833806	10.482189	-0.050115	4.815545
238.921503	7999.844739	10.487194	-0.050105	4.815548
238.903260	7999.932019	10.492199	-0.050102	4.815574
238.847930	7999.867074	10.497203	-0.050092	4.815555
239.012959	7999.830271	10.502208	-0.050123	4.815543
238.975923	7999.920448	10.507213	-0.050117	4.815570
238.870200	7999.873904	10.512218	-0.050097	4.815557
239.038494	7999.930049	10.517223	-0.050129	4.815572
238.984335	7999.829887	10.522227	-0.050119	4.815543
239.004238	7999.827028	10.527232	-0.050123	4.815542
239.018027	7999.984232	10.532237	-0.050126	4.815588
239.081255	7999.811237	10.537242	-0.050137	4.815537
239.025226	7999.923528	10.542247	-0.050127	4.815571
238.951999	7999.866834	10.547251	-0.050114	4.815554
239.067779	7999.836705	10.552256	-0.050136	4.815545
238.991705	7999.927315	10.557261	-0.050122	4.815572
238.964577	7999.821186	10.562266	-0.050117	4.815541
239.002747	7999.951025	10.567271	-0.050124	4.815579
238.928296	7999.839856	10.572275	-0.050111	4.815547
239.125436	7999.865506	10.577280	-0.050148	4.815553
239.094548	7999.845804	10.582285	-0.050142	4.815547
238.997168	7999.833563	10.587290	-0.050124	4.815544
239.018411	7999.919349	10.592295	-0.050128	4.815569
239.188366	7999.912524	10.597299	-0.050160	4.815567
239.443977	7999.864382	10.602304	-0.050208	4.815551
239.196122	7999.864642	10.607309	-0.050162	4.815552
238.983940	7999.875092	10.612314	-0.050123	4.815557
239.135240	7999.906402	10.617319	-0.050151	4.815565
239.105436	7999.890989	10.622323	-0.050146	4.815561
239.200648	7999.816747	10.627328	-0.050164	4.815538
239.059890	7999.922322	10.632333	-0.050138	4.815570
239.143380	7999.880990	10.637338	-0.050154	4.815557
239.347286	7999.852294	10.642343	-0.050192	4.815548
239.084006	7999.903555	10.647347	-0.050143	4.815564
239.182798	7999.816559	10.652352	-0.050162	4.815538
239.424395	7999.940098	10.657357	-0.050207	4.815573
239.218174	7999.886579	10.662362	-0.050169	4.815559
239.390917	7999.854173	10.667367	-0.050201	4.815548
239.097252	7999.896398	10.672371	-0.050147	4.815562
239.312591	7999.834787	10.677376	-0.050187	4.815543
239.129884	7999.926867	10.682381	-0.050153	4.815571
239.043930	7999.839001	10.687386	-0.050138	4.815546
239.471400	7999.851312	10.692391	-0.050217	4.815547
239.087872	7999.901686	10.697395	-0.050146	4.815564
238.987618	7999.902211	10.702400	-0.050128	4.815564
239.200154	7999.877926	10.707405	-0.050168	4.815556
239.242291	7999.877564	10.712410	-0.050176	4.815556
239.457304	7999.826626	10.717415	-0.050216	4.815540
239.320854	7999.891696	10.722419	-0.050191	4.815560
239.332452	7999.866279	10.727424	-0.050193	4.815552
239.096476	7999.811209	10.732429	-0.050149	4.815537
239.299241	7999.913828	10.737434	-0.050187	4.815566
239.400537	7999.830075	10.742439	-0.050206	4.815541
239.236486	7999.824224	10.747443	-0.050176	4.815540
239.165300	7999.925591	10.752448	-0.050163	4.815570
239.207309	7999.819519	10.757453	-0.050171	4.815539
239.299378	7999.887238	10.762458	-0.050189	4.815558
239.240679	7999.856406	10.767463	-0.050178	4.815550
239.105041	7999.899066	10.772467	-0.050153	4.815563
239.340611	7999.790804	10.777472	-0.050197	4.815530
239.393212	7999.906998	10.782477	-0.050207	4.815564
239.116477	7999.887568	10.787482	-0.050156	4.815559
239.362376	7999.829658	10.792487	-0.050202	4.815541
239.238628	7999.918425	10.797491	-0.050179	4.815568
239.107102	7999.856511	10.802496	-0.050155	4.815550
239.128353	7999.910265	10.807501	-0.050159	4.815566
239.337651	7999.815456	10.812506	-0.050198	4.815537
239.215145	7999.908514	10.817511	-0.050175	4.815565
239.331404	7999.876257	10.822515	-0.050197	4.815555
239.315953	7999.869620	10.827520	-0.050195	4.815553
239.203820	7999.910527	10.832525	-0.050174	4.815566
239.272858	7999.859350	10.837530	-0.050187	4.815550
239.431432	7999.892914	10.842535	-0.050217	4.815559
239.199486	7999.883823	10.847539	-0.050174	4.815558
239.133486	7999.873160	10.852544	-0.050162	4.815555
239.334226	7999.843345	10.857549	-0.050199	4.815545
239.445938	7999.882554	10.862554	-0.050221	4.815556
239.517621	7999.816471	10.867559	-0.050234	4.815537
239.214709	7999.910866	10.872563	-0.050178	4.815566
239.325103	7999.832600	10.877568	-0.050199	4.815542
239.299140	7999.940042	10.882573	-0.050194	4.815574
239.204338	7999.887268	10.887578	-0.050177	4.815559
239.316657	7999.888047	10.892583	-0.050198	4.815558
239.445595	7999.900843	10.897587	-0.050222	4.815562
239.469835	7999.826514	10.902592	-0.050227	4.815540
239.302192	7999.911364	10.907597	-0.050196	4.815565
239.415405	7999.903616	10.912602	-0.050217	4.815562
239.231855	7999.839788	10.917607	-0.050183	4.815545
239.445589	7999.832607	10.922611	-0.050223	4.815542
239.606402	7999.945224	10.927616	-0.050253	4.815574
239.384325	7999.841261	10.932621	-0.050212	4.815544
239.336681	7999.862929	10.937626	-0.050204	4.815551
239.274903	7999.926011	10.942631	-0.050192	4.815570
239.315333	7999.904266	10.947635	-0.050200	4.815563
239.315233	7999.853032	10.952640	-0.050200	4.815548
239.244043	7999.880724	10.957645	-0.050187	4.815557
239.515387	7999.858464	10.962650	-0.050238	4.815549
239.324166	7999.883135	10.967655	-0.050203	4.815557
239.432510	7999.963933	10.972659	-0.050223	4.815580
239.412841	7999.815214	10.977664	-0.050220	4.815537
239.588818	7999.921670	10.982669	-0.050253	4.815567
239.571637	7999.855209	10.987674	-0.050250	4.815547
239.578697	7999.943969	10.992679	-0.050251	4.815573
239.517783	7999.887474	10.997683	-0.050240	4.815557
239.411578	7999.859073	11.002688	-0.050221	4.815549
239.477416	7999.846283	11.007693	-0.050233	4.815545
239.582979	7999.928104	11.012698	-0.050253	4.815569
239.384775	7999.867240	11.017703	-0.050216	4.815552
239.352636	7999.815485	11.022707	-0.050211	4.815537
239.514654	7999.920646	11.027712	-0.050241	4.815567
239.416869	7999.844332	11.032717	-0.050223	4.815545
239.345959	7999.874164	11.037722	-0.050210	4.815554
239.564970	7999.856392	11.042727	-0.050251	4.815548
239.682004	7999.887146	11.047731	-0.050273	4.815556
239.724040	7999.915612	11.052736	-0.050281	4.815564
239.698805	7999.829800	11.057741	-0.050277	4.815539
239.709656	7999.898334	11.062746	-0.050279	4.815559
239.803539	7999.866781	11.067751	-0.050297	4.815550
239.599811	7999.901927	11.072755	-0.050259	4.815561
239.724015	7999.852715	11.077760	-0.050282	4.815546
239.751198	7999.910837	11.082765	-0.050288	4.815563
239.452663	7999.809902	11.087770	-0.050232	4.815535
239.559241	7999.901348	11.092775	-0.050252	4.815561
239.556356	7999.792409	11.097779	-0.050252	4.815529
239.675201	7999.866971	11.102784	-0.050274	4.815550
239.438264	7999.906915	11.107789	-0.050231	4.815563
239.538198	7999.853037	11.112794	-0.050249	4.815547
239.610963	7999.949273	11.117799	-0.050263	4.815575
239.535187	7999.804980	11.122803	-0.050249	4.815533
239.673602	7999.879860	11.127808	-0.050275	4.815554
239.857295	7999.907428	11.132813	-0.050310	4.815561
239.674356	7999.819050	11.137818	-0.050276	4.815536
239.720969	7999.946894	11.142823	-0.050285	4.815573
239.567281	7999.877144	11.147827	-0.050256	4.815554
239.888552	7999.819392	11.152832	-0.050316	4.815535
239.760938	7999.897419	11.157837	-0.050293	4.815559
239.730363	7999.862773	11.162842	-0.050287	4.815549
239.974845	7999.865704	11.167847	-0.050333	4.815548
239.777284	7999.823002	11.172851	-0.050297	4.815537
239.833238	7999.842085	11.177856	-0.050307	4.815542
239.807241	7999.936714	11.182861	-0.050303	4.815570
239.780413	7999.864757	11.187866	-0.050298	4.815549
239.630328	7999.880488	11.192871	-0.050270	4.815554
239.569542	7999.862435	11.197875	-0.050259	4.815549
239.763302	7999.947826	11.202880	-0.050295	4.815573
239.690745	7999.812126	11.207885	-0.050282	4.815534
239.563752	7999.869876	11.212890	-0.050259	4.815552
239.633141	7999.897719	11.217895	-0.050272	4.815559
239.646042	7999.881933	11.222899	-0.050275	4.815555
239.861797	7999.851295	11.227904	-0.050315	4.815545
239.908578	7999.841398	11.232909	-0.050324	4.815542
239.582825	7999.799815	11.237914	-0.050263	4.815531
239.926335	7999.945303	11.242919	-0.050328	4.815572
239.735877	7999.886700	11.247923	-0.050292	4.815556
239.800344	7999.816228	11.252928	-0.050305	4.815535
239.612534	7999.922106	11.257933	-0.050270	4.815567
239.679392	7999.857012	11.262938	-0.050283	4.815547
239.752419	7999.841136	11.267943	-0.050296	4.815542
239.625340	7999.908494	11.272947	-0.050273	4.815562
239.664097	7999.870705	11.277952	-0.050280	4.815551
239.591002	7999.926128	11.282957	-0.050267	4.815568
239.818874	7999.831620	11.287962	-0.050310	4.815539
239.688905	7999.871169	11.292967	-0.050286	4.815551
239.502119	7999.826508	11.297971	-0.050251	4.815539
239.690120	7999.888314	11.302976	-0.050286	4.815556
239.842048	7999.927111	11.307981	-0.050315	4.815567
239.665786	7999.877281	11.312986	-0.050282	4.815553
239.788620	7999.845131	11.317991	-0.050305	4.815543
239.627870	7999.899128	11.322995	-0.050276	4.815560
239.779663	7999.804451	11.328000	-0.050304	4.815531
239.775873	7999.909051	11.333005	-0.050304	4.815562
239.673613	7999.816647	11.338010	-0.050285	4.815535
239.611778	7999.873321	11.343015	-0.050274	4.815552
239.683537	7999.912949	11.348019	-0.050287	4.815563
239.774972	7999.847187	11.353024	-0.050305	4.815544
239.603852	7999.862575	11.358029	-0.050273	4.815549
239.469108	7999.941554	11.363034	-0.050248	4.815573
239.722192	7999.821830	11.368039	-0.050295	4.815537
239.668460	7999.891449	11.373043	-0.050286	4.815557
239.740757	7999.837122	11.378048	-0.050299	4.815541
239.785514	7999.851751	11.383053	-0.050308	4.815545
239.681326	7999.875703	11.388058	-0.050289	4.815552
239.867482	7999.873413	11.393063	-0.050324	4.815551
239.797515	7999.888312	11.398067	-0.050311	4.815556
239.949683	7999.858775	11.403072	-0.050339	4.815546
239.753474	7999.908992	11.408077	-0.050303	4.815562
239.705538	7999.827081	11.413082	-0.050294	4.815538
239.810147	7999.927039	11.418087	-0.050314	4.815567
239.522223	7999.938391	11.423091	-0.050261	4.815572
239.577716	7999.879519	11.428096	-0.050271	4.815554
239.521252	7999.913857	11.433101	-0.050261	4.815564
239.734371	7999.835126	11.438106	-0.050301	4.815540
239.713240	7999.902072	11.443111	-0.050297	4.815560
239.926842	7999.820146	11.448115	-0.050337	4.815535
240.098792	7999.834710	11.453120	-0.050369	4.815538
239.830545	7999.942482	11.458125	-0.050320	4.815571
239.625051	7999.891109	11.463130	-0.050282	4.815557
239.835281	7999.911634	11.468135	-0.050321	4.815562
239.879383	7999.888881	11.473139	-0.050330	4.815555
239.940647	7999.880288	11.478144	-0.050341	4.815552
239.776312	7999.880838	11.483149	-0.050311	4.815553
239.798037	7999.821416	11.488154	-0.050315	4.815536
239.880350	7999.944503	11.493159	-0.050331	4.815572
239.705453	7999.848781	11.498163	-0.050298	4.815544
239.843470	7999.857453	11.503168	-0.050324	4.815546
239.793391	7999.856658	11.508173	-0.050315	4.815546
239.692620	7999.944733	11.513178	-0.050297	4.815572
239.749835	7999.865600	11.518183	-0.050308	4.815549
239.663989	7999.828988	11.523187	-0.050292	4.815539
239.748273	7999.867751	11.528192	-0.050308	4.815550
239.629079	7999.957661	11.533197	-0.050286	4.815577
239.842958	7999.834096	11.538202	-0.050326	4.815539
239.916898	7999.938894	11.543207	-0.050340	4.815570
239.939511	7999.843182	11.548211	-0.050344	4.815542
240.088138	7999.852027	11.553216	-0.050372	4.815543
240.003030	7999.919001	11.558221	-0.050357	4.815563
239.953361	7999.815706	11.563226	-0.050348	4.815533
239.858702	7999.856897	11.568231	-0.050330	4.815546
239.843835	7999.922878	11.573235	-0.050328	4.815565
239.816205	7999.825281	11.578240	-0.050323	4.815537
239.808423	7999.888173	11.583245	-0.050322	4.815555
239.758788	7999.827591	11.588250	-0.050312	4.815538
240.038646	7999.865266	11.593255	-0.050365	4.815547
239.720805	7999.883605	11.598259	-0.050306	4.815554
239.803158	7999.837983	11.603264	-0.050321	4.815541
239.802721	7999.837997	11.608269	-0.050322	4.815541
239.708825	7999.900556	11.613274	-0.050304	4.815559
239.988811	7999.842133	11.618279	-0.050357	4.815541
239.800854	7999.907433	11.623283	-0.050322	4.815561
239.767715	7999.834305	11.628288	-0.050316	4.815540
239.786559	7999.804734	11.633293	-0.050320	4.815531
239.807417	7999.895855	11.638298	-0.050324	4.815557
239.954910	7999.869445	11.643303	-0.050352	4.815549
239.750299	7999.887492	11.648307	-0.050314	4.815555
239.986207	7999.840097	11.653312	-0.050358	4.815540
239.883191	7999.873678	11.658317	-0.050339	4.815551
239.896017	7999.901669	11.663322	-0.050342	4.815559
240.028937	7999.854734	11.668327	-0.050367	4.815544
240.008939	7999.822396	11.673331	-0.050363	4.815535
240.161881	7999.923141	11.678336	-0.050392	4.815564
239.919176	7999.859416	11.683341	-0.050347	4.815546
239.898725	7999.851629	11.688346	-0.050343	4.815544
239.925855	7999.857430	11.693351	-0.050348	4.815546
239.882280	7999.944299	11.698355	-0.050341	4.815571
239.817922	7999.876002	11.703360	-0.050329	4.815552
239.860411	7999.850019	11.708365	-0.050337	4.815544
239.965918	7999.903010	11.713370	-0.050357	4.815559
240.050048	7999.828587	11.718375	-0.050373	4.815537
240.064319	7999.833110	11.723379	-0.050376	4.815538
240.026444	7999.870955	11.728384	-0.050369	4.815549
239.978026	7999.941729	11.733389	-0.050360	4.815570
239.977035	7999.823209	11.738394	-0.050360	4.815535
239.960952	7999.907322	11.743399	-0.050357	4.815560
239.999638	7999.852447	11.748403	-0.050365	4.815544
239.861439	7999.863032	11.753408	-0.050339	4.815547
240.017136	7999.932857	11.758413	-0.050369	4.815567
239.803052	7999.820480	11.763418	-0.050329	4.815535
240.018370	7999.899816	11.768423	-0.050369	4.815557
239.980318	7999.860777	11.773427	-0.050362	4.815546
240.142070	7999.884785	11.778432	-0.050393	4.815552
240.122176	7999.859922	11.783437	-0.050389	4.815545
240.120138	7999.875926	11.788442	-0.050389	4.815550
240.063673	7999.895316	11.793447	-0.050379	4.815556
239.941601	7999.886943	11.798451	-0.050356	4.815554
239.894803	7999.906490	11.803456	-0.050348	4.815560
239.955185	7999.948068	11.808461	-0.050359	4.815572
239.892522	7999.799715	11.813466	-0.050348	4.815529
239.982619	7999.884488	11.818471	-0.050365	4.815553
240.117276	7999.940089	11.823475	-0.050390	4.815569
240.106233	7999.886541	11.828480	-0.050388	4.815553
239.972263	7999.871567	11.833485	-0.050364	4.815549
239.920907	7999.853668	11.838490	-0.050354	4.815544
240.097921	7999.903551	11.843495	-0.050388	4.815558
239.989811	7999.872982	11.848499	-0.050368	4.815550
240.052928	7999.844131	11.853504	-0.050380	4.815541
240.135390	7999.969357	11.858509	-0.050395	4.815577
240.019469	7999.917305	11.863514	-0.050374	4.815562
239.862735	7999.916910	11.868519	-0.050345	4.815563
239.963369	7999.887602	11.873523	-0.050364	4.815554
240.152762	7999.918467	11.878528	-0.050399	4.815562
240.078611	7999.893789	11.883533	-0.050386	4.815555
240.131721	7999.894674	11.888538	-0.050396	4.815555
240.235997	7999.902798	11.893543	-0.050416	4.815557
240.237966	7999.881494	11.898547	-0.050416	4.815551
240.110397	7999.886913	11.903552	-0.050393	4.815553
240.309759	7999.831449	11.908557	-0.050430	4.815536
240.058959	7999.834863	11.913562	-0.050383	4.815538
240.147296	7999.890778	11.918567	-0.050400	4.815554
240.198273	7999.887357	11.923571	-0.050410	4.815553
240.063615	7999.904406	11.928576	-0.050385	4.815558
240.048542	7999.902045	11.933581	-0.050383	4.815558
240.123103	7999.896872	11.938586	-0.050397	4.815556
240.232689	7999.899744	11.943591	-0.050417	4.815556
240.014620	7999.937859	11.948595	-0.050377	4.815568
240.077774	7999.868433	11.953600	-0.050389	4.815548
240.204920	7999.876929	11.958605	-0.050413	4.815550
240.137535	7999.880124	11.963610	-0.050400	4.815551
240.078975	7999.884530	11.968615	-0.050390	4.815552
240.127732	7999.849039	11.973619	-0.050399	4.815542
240.182508	7999.868103	11.978624	-0.050410	4.815547
240.048269	7999.855261	11.983629	-0.050385	4.815544
239.991651	7999.888530	11.988634	-0.050374	4.815554
240.170027	7999.916012	11.993639	-0.050408	4.815561
240.148991	7999.835606	11.998643	-0.050404	4.815538
240.078920	7999.872926	12.003648	-0.050391	4.815549
240.020850	7999.872001	12.008653	-0.050381	4.815549
240.041786	7999.821109	12.013658	-0.050385	4.815534
240.104402	7999.883012	12.018663	-0.050397	4.815552
240.046688	7999.952567	12.023667	-0.050386	4.815572
240.045989	7999.877831	12.028672	-0.050386	4.815551
240.038195	7999.884131	12.033677	-0.050385	4.815552
239.893873	7999.840159	12.038682	-0.050359	4.815540
240.063005	7999.881372	12.043687	-0.050390	4.815552
239.962748	7999.927811	12.048691	-0.050372	4.815566
240.110570	7999.867238	12.053696	-0.050400	4.815547
240.280016	7999.848660	12.058701	-0.050431	4.815541
240.087219	7999.822051	12.063706	-0.050396	4.815534
240.014319	7999.874275	12.068711	-0.050382	4.815550
240.081683	7999.941594	12.073715	-0.050395	4.815569
240.235486	7999.864033	12.078720	-0.050424	4.815546
240.156395	7999.865970	12.083725	-0.050410	4.815547
239.946522	7999.867914	12.088730	-0.050371	4.815548
240.083267	7999.925684	12.093735	-0.050396	4.815564
240.029363	7999.879980	12.098739	-0.050387	4.815551
240.025127	7999.857508	12.103744	-0.050386	4.815545
240.092825	7999.882121	12.108749	-0.050399	4.815552
240.025002	7999.853276	12.113754	-0.050386	4.815543
240.055482	7999.890097	12.118759	-0.050392	4.815554
239.946257	7999.916102	12.123763	-0.050372	4.815562
240.035316	7999.773421	12.128768	-0.050389	4.815520
240.152417	7999.926972	12.133773	-0.050411	4.815564
240.258736	7999.830486	12.138778	-0.050431	4.815536
240.277079	7999.899144	12.143783	-0.050435	4.815556
240.094731	7999.851349	12.148787	-0.050401	4.815542
240.069883	7999.939592	12.153792	-0.050397	4.815568
240.081108	7999.871456	12.158797	-0.050399	4.815548
240.285953	7999.866268	12.163802	-0.050437	4.815546
240.229987	7999.863242	12.168807	-0.050427	4.815545
240.098334	7999.845103	12.173811	-0.050403	4.815541
240.184657	7999.870019	12.178816	-0.050419	4.815547
240.031987	7999.958317	12.183821	-0.050391	4.815574
240.214329	7999.885492	12.188826	-0.050425	4.815552
240.209421	7999.905720	12.193831	-0.050425	4.815558
240.303569	7999.888053	12.198835	-0.050442	4.815552
240.126959	7999.915097	12.203840	-0.050410	4.815561
240.157296	7999.910272	12.208845	-0.050416	4.815559
240.149157	7999.887736	12.213850	-0.050414	4.815553
240.206043	7999.887614	12.218855	-0.050425	4.815552
240.168010	7999.873134	12.223859	-0.050418	4.815548
240.297667	7999.897689	12.228864	-0.050443	4.815555
240.105035	7999.913794	12.233869	-0.050407	4.815561
240.050367	7999.831773	12.238874	-0.050397	4.815537
240.050780	7999.873444	12.243879	-0.050397	4.815549
240.082880	7999.881461	12.248883	-0.050404	4.815551
240.226863	7999.944689	12.253888	-0.050431	4.815569
240.065641	7999.886560	12.258893	-0.050401	4.815553
240.172095	7999.863753	12.263898	-0.050421	4.815546
240.228053	7999.911667	12.268903	-0.050432	4.815559
240.255332	7999.867284	12.273907	-0.050437	4.815546
240.330159	7999.861048	12.278912	-0.050451	4.815544
240.468476	7999.903896	12.283917	-0.050477	4.815556
240.096055	7999.842330	12.288922	-0.050408	4.815540
240.148319	7999.897658	12.293927	-0.050418	4.815556
240.203640	7999.843053	12.298931	-0.050428	4.815539
240.194806	7999.936896	12.303936	-0.050427	4.815567
240.273626	7999.875199	12.308941	-0.050442	4.815548
240.342625	7999.864596	12.313946	-0.050455	4.815545
240.472006	7999.915841	12.318951	-0.050479	4.815559
240.297142	7999.847880	12.323955	-0.050447	4.815540
240.308528	7999.905746	12.328960	-0.050449	4.815557
240.386970	7999.892094	12.333965	-0.050464	4.815553
240.266084	7999.829283	12.338970	-0.050442	4.815535
240.383488	7999.858977	12.343975	-0.050464	4.815543
240.185149	7999.888871	12.348979	-0.050427	4.815553
240.222799	7999.853199	12.353984	-0.050434	4.815542
240.336660	7999.967191	12.358989	-0.050456	4.815575
240.300254	7999.832076	12.363994	-0.050449	4.815536
240.262263	7999.880597	12.368999	-0.050443	4.815550
240.188321	7999.855922	12.374003	-0.050429	4.815543
240.393728	7999.892387	12.379008	-0.050467	4.815553
240.490179	7999.883299	12.384013	-0.050486	4.815550
240.375729	7999.867576	12.389018	-0.050465	4.815546
240.234870	7999.889863	12.394023	-0.050439	4.815553
240.295210	7999.868441	12.399027	-0.050450	4.815546
240.263281	7999.943756	12.404032	-0.050444	4.815568
240.233650	7999.886700	12.409037	-0.050439	4.815552
240.210530	7999.825480	12.414042	-0.050435	4.815534
240.357694	7999.900506	12.419047	-0.050463	4.815555
240.256920	7999.870055	12.424051	-0.050444	4.815547
240.470814	7999.861811	12.429056	-0.050484	4.815543
240.510407	7999.892374	12.434061	-0.050492	4.815552
240.366097	7999.934893	12.439066	-0.050465	4.815565
240.377310	7999.899859	12.444071	-0.050467	4.815555
240.390687	7999.868063	12.449075	-0.050470	4.815546
240.413214	7999.886602	12.454080	-0.050475	4.815551
240.268473	7999.879996	12.459085	-0.050448	4.815550
240.384182	7999.862679	12.464090	-0.050470	4.815544
240.480614	7999.903778	12.469095	-0.050488	4.815556
240.339145	7999.853444	12.474099	-0.050462	4.815542
240.249414	7999.863750	12.479104	-0.050445	4.815545
240.423464	7999.929603	12.484109	-0.050478	4.815563
240.287428	7999.868681	12.489114	-0.050453	4.815546
240.205602	7999.896200	12.494119	-0.050438	4.815555
240.323399	7999.858629	12.499123	-0.050460	4.815543
240.428625	7999.909480	12.504128	-0.050480	4.815557
240.270850	7999.891984	12.509133	-0.050451	4.815553
240.220033	7999.854872	12.514138	-0.050441	4.815542
240.576716	7999.889528	12.519143	-0.050508	4.815551
240.200167	7999.869538	12.524147	-0.050438	4.815547
240.264448	7999.882350	12.529152	-0.050450	4.815550
240.257091	7999.875844	12.534157	-0.050449	4.815548
240.307076	7999.878814	12.539162	-0.050459	4.815549
240.434649	7999.915080	12.544167	-0.050483	4.815559
240.403176	7999.875079	12.549171	-0.050477	4.815547
240.373099	7999.870339	12.554176	-0.050472	4.815546
240.522093	7999.871717	12.559181	-0.050500	4.815546
240.559062	7999.933204	12.564186	-0.050507	4.815564
240.483863	7999.856186	12.569191	-0.050493	4.815542
240.285064	7999.875394	12.574195	-0.050456	4.815548
240.396607	7999.858010	12.579200	-0.050477	4.815542
240.565870	7999.876802	12.584205	-0.050509	4.815547
240.401815	7999.842118	12.589210	-0.050479	4.815538
240.335426	7999.905126	12.594215	-0.050467	4.815557
240.268472	7999.830379	12.599219	-0.050454	4.815535
240.361479	7999.846862	12.604224	-0.050472	4.815539
240.348113	7999.903258	12.609229	-0.050470	4.815556
240.169687	7999.857662	12.614234	-0.050437	4.815543
240.362318	7999.876835	12.619239	-0.050473	4.815548
240.246656	7999.930498	12.624243	-0.050452	4.815564
240.276083	7999.826353	12.629248	-0.050457	4.815534
240.290179	7999.858637	12.634253	-0.050460	4.815543
240.329284	7999.856090	12.639258	-0.050468	4.815542
240.508292	7999.860092	12.644263	-0.050501	4.815542
240.406556	7999.842439	12.649267	-0.050482	4.815538
240.475889	7999.893775	12.654272	-0.050496	4.815552
240.560416	7999.893035	12.659277	-0.050512	4.815552
240.528266	7999.926702	12.664282	-0.050506	4.815562
240.643010	7999.878403	12.669287	-0.050527	4.815547
240.360661	7999.846065	12.674291	-0.050475	4.815539
240.275683	7999.838296	12.679296	-0.050459	4.815537
240.382062	7999.859268	12.684301	-0.050479	4.815543
240.390828	7999.879719	12.689306	-0.050481	4.815549
240.585367	7999.892516	12.694311	-0.050518	4.815552
240.331708	7999.859577	12.699315	-0.050471	4.815543
240.604931	7999.906757	12.704320	-0.050522	4.815556
240.532850	7999.904536	12.709325	-0.050509	4.815555
240.469683	7999.900324	12.714330	-0.050497	4.815554
240.615530	7999.925143	12.719335	-0.050525	4.815561
240.614045	7999.850393	12.724339	-0.050525	4.815539
240.661608	7999.871475	12.729344	-0.050534	4.815545
240.659589	7999.979312	12.734349	-0.050534	4.815577
240.452840	7999.874525	12.739354	-0.050495	4.815547
240.366276	7999.923323	12.744359	-0.050479	4.815562
240.455638	7999.858594	12.749363	-0.050496	4.815542
240.305401	7999.850830	12.754368	-0.050468	4.815541
240.374786	7999.864793	12.759373	-0.050482	4.815544
240.292222	7999.811148	12.764378	-0.050466	4.815529
240.407426	7999.863229	12.769383	-0.050488	4.815544
240.378802	7999.945005	12.774387	-0.050483	4.815568
240.433415	7999.853015	12.779392	-0.050493	4.815541
240.245716	7999.896964	12.784397	-0.050459	4.815554
240.337721	7999.863244	12.789402	-0.050476	4.815544
240.339638	7999.864363	12.794407	-0.050477	4.815544
240.237528	7999.863790	12.799411	-0.050458	4.815545
240.336489	7999.878234	12.804416	-0.050477	4.815548
240.597123	7999.862208	12.809421	-0.050525	4.815542
240.261269	7999.899474	12.814426	-0.050463	4.815555
240.428653	7999.871253	12.819431	-0.050494	4.815546
240.442636	7999.830924	12.824435	-0.050497	4.815534
240.524334	7999.845088	12.829440	-0.050513	4.815538
240.474164	7999.907292	12.834445	-0.050504	4.815556
240.330794	7999.883623	12.839450	-0.050477	4.815550
240.391456	7999.882495	12.844455	-0.050489	4.815549
240.358254	7999.857415	12.849459	-0.050483	4.815542
240.308014	7999.902533	12.854464	-0.050474	4.815556
240.440144	7999.886552	12.859469	-0.050498	4.815550
240.345575	7999.924541	12.864474	-0.050481	4.815562
240.505276	7999.898331	12.869479	-0.050511	4.815553
240.466501	7999.833652	12.874483	-0.050504	4.815535
240.321788	7999.871893	12.879488	-0.050477	4.815547
240.364628	7999.865136	12.884493	-0.050486	4.815544
240.329211	7999.866715	12.889498	-0.050479	4.815545
240.633200	7999.873819	12.894503	-0.050536	4.815546
240.367539	7999.834278	12.899507	-0.050487	4.815535
240.344285	7999.848869	12.904512	-0.050483	4.815540
240.620573	7999.873675	12.909517	-0.050534	4.815546
240.352364	7999.851177	12.914522	-0.050485	4.815540
240.374209	7999.892129	12.919527	-0.050489	4.815552
240.417446	7999.861887	12.924531	-0.050497	4.815543
240.347675	7999.940857	12.929536	-0.050485	4.815567
240.434746	7999.826972	12.934541	-0.050501	4.815533
240.573370	7999.894385	12.939546	-0.050527	4.815552
240.544626	7999.890734	12.944551	-0.050522	4.815551
240.415065	7999.873696	12.949555	-0.050498	4.815547
240.506508	7999.858120	12.954560	-0.050515	4.815542
240.643822	7999.895613	12.959565	-0.050541	4.815552
240.518635	7999.826324	12.964570	-0.050518	4.815532
240.606112	7999.888633	12.969575	-0.050534	4.815550
240.558277	7999.882535	12.974579	-0.050526	4.815548
240.633763	7999.860293	12.979584	-0.050540	4.815542
240.570289	7999.846466	12.984589	-0.050528	4.815538
240.736352	7999.918597	12.989594	-0.050560	4.815558
240.748714	7999.892124	12.994599	-0.050562	4.815550
240.484198	7999.854736	12.999603	-0.050513	4.815541
240.530781	7999.893956	13.004608	-0.050522	4.815552
240.552739	7999.895401	13.009613	-0.050526	4.815552
240.297763	7999.864576	13.014618	-0.050479	4.815544
240.377077	7999.908599	13.019623	-0.050494	4.815557
240.404570	7999.885576	13.024627	-0.050499	4.815550
240.441359	7999.871245	13.029632	-0.050507	4.815546
240.436903	7999.881871	13.034637	-0.050506	4.815549
240.359690	7999.856075	13.039642	-0.050492	4.815542
240.487334	7999.909428	13.044647	-0.050516	4.815557
240.556715	7999.872137	13.049651	-0.050529	4.815545
240.509150	7999.841484	13.054656	-0.050520	4.815537
240.528616	7999.851432	13.059661	-0.050524	4.815539
240.376242	7999.922650	13.064666	-0.050496	4.815561
240.463980	7999.880319	13.069671	-0.050513	4.815548
240.554494	7999.860456	13.074675	-0.050530	4.815542
240.572864	7999.951539	13.079680	-0.050533	4.815568
240.346981	7999.916916	13.084685	-0.050492	4.815559
240.444411	7999.889692	13.089690	-0.050510	4.815551
240.779777	7999.936816	13.094695	-0.050573	4.815563
240.467995	7999.885845	13.099699	-0.050515	4.815550
240.338235	7999.873075	13.104704	-0.050491	4.815547
240.490807	7999.870240	13.109709	-0.050519	4.815545
240.442490	7999.867338	13.114714	-0.050511	4.815544
240.632354	7999.890738	13.119719	-0.050546	4.815550
240.465961	7999.888049	13.124723	-0.050516	4.815550
240.546585	7999.879772	13.129728	-0.050531	4.815547
240.604877	7999.889283	13.134733	-0.050542	4.815550
240.465369	7999.840049	13.139738	-0.050516	4.815536
240.642847	7999.914502	13.144743	-0.050549	4.815557
240.625910	7999.890755	13.149747	-0.050547	4.815550
240.418065	7999.941850	13.154752	-0.050508	4.815566
240.717994	7999.904040	13.159757	-0.050564	4.815554
240.659658	7999.889229	13.164762	-0.050553	4.815550
240.683473	7999.936621	13.169767	-0.050558	4.815563
240.442934	7999.882539	13.174771	-0.050514	4.815549
240.450177	7999.904033	13.179776	-0.050515	4.815555
240.365094	7999.888787	13.184781	-0.050500	4.815551
240.275386	7999.847838	13.189786	-0.050483	4.815539
240.533075	7999.909715	13.194791	-0.050531	4.815556
240.589189	7999.875411	13.199795	-0.050542	4.815546
240.634765	7999.858020	13.204800	-0.050551	4.815541
240.606871	7999.881078	13.209805	-0.050546	4.815547
240.606610	7999.860806	13.214810	-0.050546	4.815542
240.653343	7999.924588	13.219815	-0.050555	4.815560
240.644081	7999.871067	13.224819	-0.050553	4.815544
240.730704	7999.862887	13.229824	-0.050570	4.815542
240.761580	7999.913597	13.234829	-0.050576	4.815556
240.433305	7999.911477	13.239834	-0.050515	4.815557
240.549452	7999.933676	13.244839	-0.050537	4.815563
240.679520	7999.885627	13.249843	-0.050561	4.815548
240.632086	7999.914774	13.254848	-0.050553	4.815557
240.596164	7999.918481	13.259853	-0.050546	4.815558
240.568385	7999.863591	13.264858	-0.050541	4.815542
240.685094	7999.905020	13.269863	-0.050563	4.815554
240.539777	7999.883454	13.274867	-0.050536	4.815548
240.878679	7999.878313	13.279872	-0.050600	4.815545
240.725818	7999.893998	13.284877	-0.050571	4.815551
240.417973	7999.840956	13.289882	-0.050514	4.815537
240.707711	7999.900150	13.294887	-0.050568	4.815552
240.640967	7999.959950	13.299891	-0.050556	4.815570
240.620687	7999.873147	13.304896	-0.050553	4.815545
240.619345	7999.892366	13.309901	-0.050553	4.815551
240.812042	7999.847472	13.314906	-0.050589	4.815537
240.618446	7999.929765	13.319911	-0.050553	4.815562
240.628424	7999.903253	13.324915	-0.050555	4.815554
240.698898	7999.868115	13.329920	-0.050568	4.815543
240.811965	7999.864637	13.334925	-0.050590	4.815542
240.672595	7999.858117	13.339930	-0.050564	4.815540
240.754065	7999.885091	13.344935	-0.050579	4.815548
240.629627	7999.871340	13.349939	-0.050556	4.815544
240.755025	7999.847774	13.354944	-0.050580	4.815537
240.726004	7999.833440	13.359949	-0.050575	4.815533
240.704205	7999.843784	13.364954	-0.050571	4.815536
240.707294	7999.906856	13.369959	-0.050572	4.815554
240.560290	7999.895940	13.374963	-0.050545	4.815552
240.544827	7999.885031	13.379968	-0.050542	4.815549
240.652269	7999.909224	13.384973	-0.050562	4.815555
240.437015	7999.839536	13.389978	-0.050522	4.815536
240.760431	7999.917433	13.394983	-0.050583	4.815557
240.771180	7999.872780	13.399987	-0.050585	4.815544
240.686640	7999.889577	13.404992	-0.050570	4.815549
240.581993	7999.902843	13.409997	-0.050550	4.815554
240.649739	7999.868728	13.415002	-0.050563	4.815543
240.733454	7999.875450	13.420007	-0.050579	4.815545
240.584616	7999.969151	13.425011	-0.050552	4.815573
240.677163	7999.862829	13.430016	-0.050569	4.815542
240.751848	7999.889692	13.435021	-0.050583	4.815549
240.662237	7999.873304	13.440026	-0.050567	4.815545
240.576473	7999.895420	13.445031	-0.050551	4.815552
240.557493	7999.901539	13.450035	-0.050548	4.815553
240.895433	7999.871823	13.455040	-0.050611	4.815543
240.851888	7999.890355	13.460045	-0.050603	4.815549
240.702642	7999.823877	13.465050	-0.050575	4.815530
240.888184	7999.899529	13.470055	-0.050610	4.815551
240.607026	7999.856531	13.475059	-0.050558	4.815540
240.780181	7999.901015	13.480064	-0.050591	4.815552
240.797659	7999.887438	13.485069	-0.050594	4.815548
240.722048	7999.838176	13.490074	-0.050580	4.815534
240.812462	7999.884516	13.495079	-0.050597	4.815547
240.746208	7999.879187	13.500083	-0.050585	4.815546
240.582767	7999.908581	13.505088	-0.050555	4.815555
240.603969	7999.856623	13.510093	-0.050559	4.815540
240.522715	7999.847846	13.515098	-0.050544	4.815538
240.711228	7999.860546	13.520103	-0.050580	4.815541
240.474833	7999.857786	13.525107	-0.050536	4.815541
240.518336	7999.833955	13.530112	-0.050544	4.815534
240.705143	7999.959814	13.535117	-0.050579	4.815570
240.552196	7999.820665	13.540122	-0.050551	4.815530
240.516146	7999.815827	13.545127	-0.050544	4.815528
240.571318	7999.833831	13.550131	-0.050555	4.815533
240.701379	7999.855189	13.555136	-0.050579	4.815539
240.741970	7999.899650	13.560141	-0.050587	4.815552
240.703765	7999.844590	13.565146	-0.050580	4.815536
240.793064	7999.902658	13.570151	-0.050597	4.815552
240.781374	7999.951608	13.575155	-0.050595	4.815567
240.776405	7999.891750	13.580160	-0.050595	4.815549
240.875524	7999.898723	13.585165	-0.050613	4.815551
240.697529	7999.849929	13.590170	-0.050580	4.815537
240.728004	7999.835496	13.595175	-0.050586	4.815533
240.719181	7999.851390	13.600179	-0.050585	4.815538
240.562592	7999.861675	13.605184	-0.050556	4.815542
240.561894	7999.899057	13.610189	-0.050556	4.815552
240.604573	7999.848518	13.615194	-0.050564	4.815537
240.765910	7999.908826	13.620199	-0.050594	4.815554
240.663234	7999.905039	13.625203	-0.050576	4.815554
240.610093	7999.918076	13.630208	-0.050566	4.815558
240.722486	7999.919926	13.635213	-0.050587	4.815558
240.860410	7999.858123	13.640218	-0.050613	4.815539
240.724341	7999.851657	13.645223	-0.050588	4.815538
240.614858	7999.869116	13.650227	-0.050568	4.815543
240.584388	7999.871844	13.655232	-0.050562	4.815544
240.844509	7999.897455	13.660237	-0.050611	4.815551
240.820357	7999.824471	13.665242	-0.050607	4.815529
240.806391	7999.864841	13.670247	-0.050604	4.815541
240.761435	7999.844908	13.675251	-0.050596	4.815536
240.697381	7999.862039	13.680256	-0.050584	4.815541
240.958677	7999.873788	13.685261	-0.050633	4.815543
240.663870	7999.890365	13.690266	-0.050579	4.815549
240.894172	7999.902677	13.695271	-0.050622	4.815552
240.744802	7999.878909	13.700275	-0.050594	4.815546
240.846088	7999.888053	13.705280	-0.050613	4.815548
240.865209	7999.861690	13.710285	-0.050617	4.815540
240.634906	7999.944453	13.715290	-0.050574	4.815565
240.738482	7999.875684	13.720295	-0.050594	4.815545
240.567107	7999.844084	13.725299	-0.050562	4.815536
240.884229	7999.916539	13.730304	-0.050622	4.815556
240.799667	7999.902369	13.735309	-0.050606	4.815552
240.664488	7999.851069	13.740314	-0.050581	4.815538
240.655167	7999.889379	13.745319	-0.050580	4.815549
240.651167	7999.866910	13.750323	-0.050579	4.815542
240.613475	7999.852435	13.755328	-0.050572	4.815538
240.820873	7999.851561	13.760333	-0.050611	4.815537
240.744241	7999.824706	13.765338	-0.050597	4.815530
240.758991	7999.842051	13.770343	-0.050600	4.815535
240.823698	7999.867685	13.775347	-0.050612	4.815542
240.774457	7999.926701	13.780352	-0.050603	4.815559
240.827144	7999.883799	13.785357	-0.050614	4.815547
240.722698	7999.876780	13.790362	-0.050594	4.815545
240.709563	7999.881925	13.795367	-0.050592	4.815547
240.957603	7999.848610	13.800371	-0.050638	4.815536
240.925817	7999.890826	13.805376	-0.050633	4.815548
240.797105	7999.848174	13.810381	-0.050609	4.815536
240.694722	7999.850798	13.815386	-0.050590	4.815537
240.729700	7999.897304	13.820391	-0.050597	4.815551
240.729588	7999.901594	13.825395	-0.050597	4.815552
240.705908	7999.918314	13.830400	-0.050593	4.815557
240.829629	7999.857347	13.835405	-0.050616	4.815539
240.862174	7999.895271	13.840410	-0.050623	4.815550
240.958288	7999.877636	13.845415	-0.050641	4.815544
240.676108	7999.864519	13.850419	-0.050588	4.815542
240.684462	7999.837980	13.855424	-0.050590	4.815534
240.685507	7999.878594	13.860429	-0.050591	4.815546
240.627957	7999.833898	13.865434	-0.050580	4.815533
240.583371	7999.760581	13.870439	-0.050572	4.815512
240.796163	7999.940255	13.875443	-0.050612	4.815563
240.662646	7999.863354	13.880448	-0.050587	4.815541
240.754014	7999.906507	13.885453	-0.050605	4.815553
240.817135	7999.884063	13.890458	-0.050617	4.815547
240.695463	7999.910933	13.895463	-0.050594	4.815555
240.707170	7999.906873	13.900467	-0.050597	4.815554
240.810649	7999.910714	13.905472	-0.050616	4.815554
240.773798	7999.887710	13.910477	-0.050609	4.815548
240.566639	7999.855527	13.915482	-0.050571	4.815539
240.731845	7999.888135	13.920487	-0.050602	4.815548
240.797465	7999.944751	13.925491	-0.050615	4.815564
240.515648	7999.880385	13.930496	-0.050562	4.815547
240.519103	7999.876190	13.935501	-0.050563	4.815546
240.797330	7999.833756	13.940506	-0.050615	4.815532
240.939636	7999.896959	13.945511	-0.050642	4.815550
240.674873	7999.862770	13.950515	-0.050593	4.815541
240.669755	7999.845622	13.955520	-0.050592	4.815536
240.700616	7999.848280	13.960525	-0.050598	4.815537
240.697709	7999.835440	13.965530	-0.050598	4.815533
240.792988	7999.891470	13.970535	-0.050616	4.815549
240.863111	7999.837105	13.975539	-0.050629	4.815532
240.735919	7999.861750	13.980544	-0.050606	4.815540
240.961176	7999.915626	13.985549	-0.050648	4.815555
240.853156	7999.919226	13.990554	-0.050628	4.815557
240.725051	7999.905415	13.995559	-0.050604	4.815553
240.596500	7999.861698	14.000563	-0.050581	4.815541
240.875539	7999.849176	14.005568	-0.050633	4.815536
240.756719	7999.899585	14.010573	-0.050611	4.815551
240.781790	7999.864775	14.015578	-0.050616	4.815541
240.760838	7999.895421	14.020583	-0.050612	4.815550
240.889903	7999.849491	14.025587	-0.050636	4.815536
240.817264	7999.864346	14.030592	-0.050623	4.815541
240.904299	7999.903157	14.035597	-0.050640	4.815552
240.783723	7999.878790	14.040602	-0.050617	4.815545
240.872027	7999.877044	14.045607	-0.050634	4.815544
240.724861	7999.859719	14.050611	-0.050607	4.815540
240.926155	7999.858746	14.055616	-0.050644	4.815538
240.777811	7999.886250	14.060621	-0.050617	4.815547
240.751915	7999.877306	14.065626	-0.050613	4.815545
240.901417	7999.800742	14.070631	-0.050641	4.815522
241.024956	7999.978964	14.075635	-0.050664	4.815573
240.831134	7999.878657	14.080640	-0.050628	4.815545
240.775744	7999.890589	14.085645	-0.050618	4.815548
240.754080	7999.855019	14.090650	-0.050614	4.815538
240.816516	7999.885954	14.095655	-0.050626	4.815547
240.724136	7999.874860	14.100659	-0.050609	4.815544
240.927709	7999.844025	14.105664	-0.050647	4.815534
241.035720	7999.900263	14.110669	-0.050667	4.815550
240.994026	7999.853688	14.115674	-0.050660	4.815537
240.885262	7999.845530	14.120679	-0.050640	4.815535
241.034941	7999.913125	14.125683	-0.050668	4.815554
241.103259	7999.857663	14.130688	-0.050681	4.815537
241.016216	7999.871216	14.135693	-0.050665	4.815542
240.978370	7999.840721	14.140698	-0.050658	4.815533
241.027607	7999.870374	14.145703	-0.050668	4.815541
240.773424	7999.874798	14.150707	-0.050620	4.815544
240.708183	7999.886570	14.155712	-0.050609	4.815547
240.887068	7999.903385	14.160717	-0.050642	4.815552
240.733537	7999.893430	14.165722	-0.050614	4.815549
240.776362	7999.913369	14.170727	-0.050622	4.815555
240.819105	7999.882051	14.175731	-0.050630	4.815546
240.805847	7999.817786	14.180736	-0.050628	4.815527
240.997149	7999.902075	14.185741	-0.050664	4.815551
240.922313	7999.856029	14.190746	-0.050650	4.815537
241.148625	7999.862937	14.195751	-0.050692	4.815538
240.849324	7999.883712	14.200755	-0.050637	4.815546
241.009069	7999.874587	14.205760	-0.050667	4.815542
241.116807	7999.904126	14.210765	-0.050687	4.815551
240.859301	7999.944801	14.215770	-0.050640	4.815564
240.977509	7999.879474	14.220775	-0.050662	4.815544
240.993199	7999.860529	14.225779	-0.050665	4.815538
241.176364	7999.829361	14.230784	-0.050699	4.815528
241.108752	7999.912639	14.235789	-0.050687	4.815553
240.825539	7999.865334	14.240794	-0.050634	4.815541
241.016784	7999.913317	14.245799	-0.050670	4.815554
241.144164	7999.637778	14.250803	-0.050694	4.815473

241.058163	7996.367089	14.255808	-0.050676	4.814517
240.974801	7990.762907	14.260813	-0.050657	4.812878
240.907836	7983.946873	14.265818	-0.050640	4.810884
240.920851	7976.675363	14.270823	-0.050638	4.808755
240.993602	7969.088255	14.275827	-0.050647	4.806533
240.835636	7961.206003	14.280832	-0.050613	4.804224
240.734793	7953.425368	14.285837	-0.050589	4.801944
240.575820	7945.374086	14.290842	-0.050555	4.799583
240.689565	7937.452129	14.295847	-0.050571	4.797258
240.595915	7929.442705	14.300851	-0.050548	4.794908
240.486072	7921.381761	14.305856	-0.050523	4.792541
240.716934	7913.351989	14.310861	-0.050561	4.790180
240.535210	7905.378712	14.315866	-0.050522	4.787837
240.311874	7897.385497	14.320871	-0.050476	4.785486
240.445393	7889.427673	14.325875	-0.050496	4.783144
240.452162	7881.395678	14.330880	-0.050492	4.780779
240.282532	7873.470227	14.335885	-0.050455	4.778445
240.146748	7865.403016	14.340890	-0.050425	4.776068
240.398250	7857.381898	14.345895	-0.050467	4.773702
240.387392	7849.333846	14.350899	-0.050460	4.771327
240.121494	7841.315190	14.355904	-0.050405	4.768962
240.135773	7833.398122	14.360909	-0.050403	4.766624
240.072769	7825.345620	14.365914	-0.050386	4.764245
240.194961	7817.442968	14.370919	-0.050404	4.761908
240.119310	7809.343441	14.375923	-0.050385	4.759513
240.172121	7801.413000	14.380928	-0.050390	4.757166
240.064127	7793.407682	14.385933	-0.050365	4.754796
239.989760	7785.285595	14.390938	-0.050346	4.752391
240.061737	7777.313543	14.395943	-0.050354	4.750028
240.058525	7769.363583	14.400947	-0.050349	4.747671
239.698670	7761.318083	14.405952	-0.050277	4.745286
239.755111	7753.368356	14.410957	-0.050282	4.742926
239.688090	7745.318313	14.415962	-0.050265	4.740536
239.709656	7737.355188	14.420967	-0.050264	4.738170
239.672719	7729.310416	14.425971	-0.050252	4.735779
239.700093	7721.319671	14.430976	-0.050252	4.733402
239.707721	7713.326458	14.435981	-0.050249	4.731024
239.431323	7705.306362	14.440986	-0.050192	4.728637
239.558068	7697.338054	14.445991	-0.050211	4.726264
239.384990	7689.282051	14.450995	-0.050173	4.723863
239.353361	7681.322507	14.456000	-0.050163	4.721490
239.307591	7673.338615	14.461005	-0.050149	4.719109
239.261085	7665.362957	14.466010	-0.050136	4.716729
239.359140	7657.313063	14.471015	-0.050149	4.714325
239.283017	7649.348424	14.476019	-0.050130	4.711945
239.167641	7641.259108	14.481024	-0.050103	4.709528
239.121819	7633.304973	14.486029	-0.050090	4.707149
238.887595	7625.256512	14.491034	-0.050041	4.704741
238.972785	7617.304177	14.496039	-0.050052	4.702361
239.048709	7609.304719	14.501043	-0.050061	4.699964
239.073519	7601.327728	14.506048	-0.050061	4.697574
238.949709	7593.335101	14.511053	-0.050033	4.695178
238.954615	7585.296430	14.516058	-0.050029	4.692766
238.897038	7577.280239	14.521063	-0.050013	4.690360
238.985136	7569.268004	14.526067	-0.050024	4.687954
238.998371	7561.275017	14.531072	-0.050022	4.685553
238.867001	7553.353869	14.536077	-0.049992	4.683172
238.737482	7545.270769	14.541082	-0.049963	4.680741
238.728761	7537.263073	14.546087	-0.049957	4.678332
238.941967	7529.322804	14.551091	-0.049991	4.675941
238.626537	7521.249333	14.556096	-0.049928	4.673509
238.755169	7513.183229	14.561101	-0.049947	4.671078
238.645014	7505.181325	14.566106	-0.049921	4.668666
238.567111	7497.231332	14.571111	-0.049902	4.666267
238.337135	7489.204212	14.576115	-0.049854	4.663845
238.256925	7481.239794	14.581120	-0.049834	4.661439
238.339951	7473.247048	14.586125	-0.049844	4.659024
238.362210	7465.265446	14.591130	-0.049844	4.656611
238.373909	7457.232226	14.596135	-0.049841	4.654181
238.476787	7449.248853	14.601139	-0.049855	4.651765
238.212052	7441.167562	14.606144	-0.049801	4.649319
238.441695	7433.276322	14.611149	-0.049838	4.646928
238.191746	7425.139759	14.616154	-0.049787	4.644462
238.300625	7417.290401	14.621159	-0.049802	4.642081
238.118374	7409.258270	14.626163	-0.049763	4.639644
238.052272	7401.245039	14.631168	-0.049746	4.637211
238.232463	7393.231302	14.636173	-0.049775	4.634777
238.033962	7385.141075	14.641178	-0.049733	4.632319
238.026841	7377.147842	14.646183	-0.049726	4.629888
237.956339	7369.179271	14.651187	-0.049708	4.627464
237.963195	7361.129867	14.656192	-0.049704	4.625014
237.900335	7353.238418	14.661197	-0.049688	4.622611
237.678843	7345.167684	14.666202	-0.049642	4.620151
237.726008	7337.210948	14.671207	-0.049645	4.617726
237.633885	7329.214378	14.676211	-0.049623	4.615286
237.633689	7321.196498	14.681216	-0.049618	4.612839
237.844129	7313.170544	14.686221	-0.049652	4.610388
237.674207	7305.178613	14.691226	-0.049616	4.607947
237.685178	7297.151039	14.696231	-0.049613	4.605493
237.537973	7289.203410	14.701235	-0.049580	4.603062
237.335763	7281.155051	14.706240	-0.049538	4.600599
237.384227	7273.201487	14.711245	-0.049542	4.598164
237.422082	7265.150254	14.716250	-0.049544	4.595698
237.481250	7257.117558	14.721255	-0.049550	4.593236
237.168527	7249.131585	14.726259	-0.049487	4.590786
237.092132	7241.125097	14.731264	-0.049468	4.588330
237.420163	7233.117947	14.736269	-0.049524	4.585872
237.339287	7225.119029	14.741274	-0.049504	4.583415
237.057061	7217.124977	14.746279	-0.049446	4.580958
237.258664	7209.146128	14.751283	-0.049479	4.578504
237.220896	7201.136709	14.756288	-0.049467	4.576040
237.012582	7193.155501	14.761293	-0.049423	4.573583
236.767573	7185.111913	14.766298	-0.049372	4.571106
237.013112	7177.110508	14.771303	-0.049413	4.568640
237.007964	7169.122392	14.776307	-0.049407	4.566177
236.615699	7161.114859	14.781312	-0.049329	4.563706
236.664673	7153.187825	14.786317	-0.049333	4.561260
236.587603	7145.164525	14.791322	-0.049314	4.558782
236.825095	7137.201753	14.796327	-0.049353	4.556322
236.743951	7129.107426	14.801331	-0.049333	4.553819
236.625606	7121.102529	14.806336	-0.049306	4.551343
236.538990	7113.074651	14.811341	-0.049285	4.548858
236.434156	7105.094638	14.816346	-0.049260	4.546387
236.456065	7097.070962	14.821351	-0.049259	4.543900
236.389640	7089.149843	14.826355	-0.049242	4.541445
236.247109	7081.101680	14.831360	-0.049211	4.538948
236.599512	7073.189725	14.836365	-0.049271	4.536493
236.448825	7065.136354	14.841370	-0.049238	4.533992
236.103303	7057.134979	14.846375	-0.049169	4.531505
236.142534	7049.102416	14.851379	-0.049171	4.529008
236.259242	7041.089794	14.856384	-0.049188	4.526517
236.290319	7033.141328	14.861389	-0.049189	4.524043
236.095176	7025.154755	14.866394	-0.049147	4.521556
236.056025	7017.128413	14.871399	-0.049135	4.519055
236.118647	7009.186854	14.876403	-0.049142	4.516579
235.992530	7001.075000	14.881408	-0.049113	4.514049
236.156996	6993.025410	14.886413	-0.049139	4.511537
236.074944	6985.018272	14.891418	-0.049119	4.509037
235.829808	6977.040973	14.896423	-0.049068	4.506544
235.621578	6969.065876	14.901427	-0.049024	4.504051
235.548870	6961.076122	14.906432	-0.049006	4.501551
235.879980	6953.080202	14.911437	-0.049062	4.499050
235.884838	6945.077669	14.916442	-0.049058	4.496544
235.990736	6937.054740	14.921447	-0.049073	4.494031
236.008446	6929.077937	14.926451	-0.049071	4.491531
235.830240	6921.042820	14.931456	-0.049033	4.489010
235.748948	6913.058067	14.936461	-0.049013	4.486504
235.654214	6905.059067	14.941466	-0.048991	4.483992
235.532598	6897.090702	14.946471	-0.048963	4.481488
235.399631	6889.049523	14.951475	-0.048933	4.478960
235.408536	6881.065989	14.956480	-0.048930	4.476449
235.635814	6873.064704	14.961485	-0.048967	4.473932
235.493729	6864.993667	14.966490	-0.048936	4.471390
235.557284	6857.062642	14.971495	-0.048943	4.468891
235.503926	6849.061151	14.976499	-0.048928	4.466369
235.451294	6841.016705	14.981504	-0.048913	4.463831
235.454925	6833.020691	14.986509	-0.048909	4.461308
235.310443	6825.013217	14.991514	-0.048877	4.458778
235.183240	6817.017053	14.996519	-0.048848	4.456251
235.173755	6809.018082	15.001523	-0.048841	4.453723
235.110797	6800.989812	15.006528	-0.048825	4.451183
235.390647	6793.020893	15.011533	-0.048872	4.448662
235.009801	6785.006909	15.016538	-0.048796	4.446122
235.022891	6777.010146	15.021543	-0.048793	4.443589
234.819305	6769.077972	15.026547	-0.048750	4.441073
234.606771	6760.985212	15.031552	-0.048706	4.438505
234.731842	6753.045931	15.036557	-0.048724	4.435985
234.614453	6744.970073	15.041562	-0.048697	4.433420
234.584913	6736.967421	15.046567	-0.048687	4.430877
234.704108	6728.992753	15.051571	-0.048704	4.428342
234.609145	6720.984549	15.056576	-0.048681	4.425794
234.729663	6712.983683	15.061581	-0.048699	4.423247
234.564878	6704.961303	15.066586	-0.048663	4.420691
234.521590	6696.986832	15.071591	-0.048650	4.418150
234.723522	6688.996547	15.076595	-0.048683	4.415603
234.580274	6680.913488	15.081600	-0.048651	4.413023
234.533351	6672.959809	15.086605	-0.048637	4.410484
234.414157	6664.980628	15.091610	-0.048610	4.407934
234.355615	6656.940687	15.096615	-0.048594	4.405364
234.355559	6649.032354	15.101619	-0.048589	4.402835
234.195251	6640.995659	15.106624	-0.048554	4.400262
234.498894	6633.025150	15.111629	-0.048606	4.397712
234.341354	6625.043608	15.116634	-0.048572	4.395154
234.303382	6616.957626	15.121639	-0.048560	4.392562
234.372707	6608.934905	15.126643	-0.048568	4.389989
234.178904	6600.976925	15.131648	-0.048526	4.387434
234.126168	6592.999776	15.136653	-0.048512	4.384872
233.987554	6585.037602	15.141658	-0.048481	4.382313
234.203252	6576.976630	15.146663	-0.048516	4.379723
234.169617	6569.051052	15.151667	-0.048505	4.377173
233.771326	6560.991427	15.156672	-0.048426	4.374576
233.875058	6553.018439	15.161677	-0.048440	4.372009
233.776457	6544.941586	15.166682	-0.048417	4.369406
233.731091	6537.006988	15.171687	-0.048403	4.366847
233.937289	6528.988047	15.176691	-0.048437	4.364261
233.730162	6521.041788	15.181696	-0.048393	4.361694
233.646298	6512.983856	15.186701	-0.048373	4.359091
233.598159	6505.047874	15.191706	-0.048359	4.356526
233.494068	6496.960415	15.196711	-0.048334	4.353909
233.372237	6488.858936	15.201715	-0.048306	4.351287
233.403727	6480.867213	15.206720	-0.048307	4.348699
233.338050	6472.919819	15.211725	-0.048290	4.346124
233.302719	6464.969797	15.216730	-0.048279	4.343547
233.499153	6456.948434	15.221735	-0.048310	4.340946
233.195210	6448.991483	15.226739	-0.048249	4.338361
233.021185	6440.974151	15.231744	-0.048211	4.335756
232.982628	6432.965505	15.236749	-0.048199	4.333153
232.998121	6424.925960	15.241754	-0.048197	4.330539
232.923013	6416.970967	15.246759	-0.048178	4.327951
233.066876	6408.946879	15.251763	-0.048200	4.325339
232.816857	6400.965160	15.256768	-0.048148	4.322737
233.049409	6392.976485	15.261773	-0.048187	4.320135
232.801776	6384.993918	15.266778	-0.048136	4.317530
232.751188	6376.949581	15.271783	-0.048121	4.314904
232.944846	6368.942734	15.276787	-0.048152	4.312291
232.663622	6360.886823	15.281792	-0.048095	4.309657
232.819974	6352.969787	15.286797	-0.048119	4.307070
232.760393	6344.897537	15.291802	-0.048103	4.304428
232.735548	6336.938134	15.296807	-0.048093	4.301823
232.845353	6328.951732	15.301811	-0.048109	4.299208
232.576642	6320.966037	15.306816	-0.048054	4.296588
232.711430	6312.952583	15.311821	-0.048074	4.293962
232.673572	6304.871215	15.316826	-0.048062	4.291310
232.456659	6296.854462	15.321831	-0.048016	4.288675
232.532773	6288.950310	15.326835	-0.048026	4.286079
232.414246	6280.907750	15.331840	-0.047999	4.283434
232.352326	6272.987366	15.336845	-0.047982	4.280828
232.161185	6264.949996	15.341850	-0.047942	4.278181
232.328356	6256.951048	15.346855	-0.047968	4.275548
232.157197	6248.930755	15.351859	-0.047931	4.272903
231.999043	6240.832824	15.356864	-0.047896	4.270232
232.146590	6232.908808	15.361869	-0.047919	4.267618
231.978896	6224.842036	15.366874	-0.047883	4.264953
231.856963	6216.941633	15.371879	-0.047855	4.262342
232.180655	6208.886791	15.376883	-0.047910	4.259682
232.179698	6200.936282	15.381888	-0.047905	4.257052
232.116984	6192.935813	15.386893	-0.047888	4.254403
231.964568	6184.890069	15.391898	-0.047855	4.251737
231.992545	6176.899040	15.396903	-0.047855	4.249089
231.907143	6168.943460	15.401907	-0.047834	4.246450
231.898930	6160.880643	15.406912	-0.047828	4.243775
231.885650	6152.940561	15.411917	-0.047821	4.241138
231.635051	6144.944584	15.416922	-0.047769	4.238479
231.571598	6136.960547	15.421927	-0.047752	4.235824
231.853067	6128.933081	15.426931	-0.047800	4.233156
231.603618	6120.885750	15.431936	-0.047748	4.230475
231.709946	6112.919379	15.436941	-0.047763	4.227823
231.549073	6104.947146	15.441946	-0.047728	4.225164
231.580959	6096.954613	15.446951	-0.047729	4.222499
231.603857	6088.887897	15.451955	-0.047728	4.219807
231.574800	6080.919485	15.456960	-0.047718	4.217146
231.555445	6072.948355	15.461965	-0.047709	4.214482
231.492684	6064.901464	15.466970	-0.047693	4.211791
231.332973	6056.896311	15.471975	-0.047658	4.209111
231.437736	6048.935691	15.476979	-0.047672	4.206447
231.401534	6040.890371	15.481984	-0.047661	4.203751
231.177124	6033.009750	15.486989	-0.047614	4.201107
230.943740	6024.930702	15.491994	-0.047565	4.198395
231.026904	6016.965961	15.496999	-0.047576	4.195723
231.233354	6008.912196	15.502003	-0.047609	4.193020
231.015426	6000.811234	15.507008	-0.047564	4.190295
230.949999	5992.912101	15.512013	-0.047547	4.187638
230.959472	5984.856058	15.517018	-0.047543	4.184927
230.644341	5976.921507	15.522023	-0.047480	4.182252
230.714341	5968.930418	15.527027	-0.047488	4.179560
230.715572	5960.901371	15.532032	-0.047483	4.176853
230.868653	5952.908564	15.537037	-0.047507	4.174158
230.676507	5944.896357	15.542042	-0.047466	4.171451
230.748310	5936.899034	15.547047	-0.047474	4.168750
230.581748	5928.942635	15.552051	-0.047438	4.166058
230.493178	5920.889151	15.557056	-0.047417	4.163333
230.815283	5912.920979	15.562061	-0.047472	4.160640
230.687589	5904.915270	15.567066	-0.047443	4.157927
230.475550	5896.920528	15.572071	-0.047399	4.155215
230.404421	5888.883864	15.577075	-0.047380	4.152488
230.473443	5880.850368	15.582080	-0.047388	4.149763
230.573089	5872.929497	15.587085	-0.047402	4.147074
230.214830	5864.854512	15.592090	-0.047330	4.144326
230.196822	5856.910605	15.597095	-0.047322	4.141624
230.184234	5848.907495	15.602099	-0.047314	4.138901
230.205767	5840.886440	15.607104	-0.047313	4.136170
230.180043	5832.878800	15.612109	-0.047304	4.133442
230.278422	5824.878362	15.617114	-0.047317	4.130715
230.211045	5816.900209	15.622119	-0.047299	4.127993
230.169484	5808.851441	15.627123	-0.047287	4.125244
229.970659	5800.898833	15.632128	-0.047245	4.122525
229.927609	5792.931170	15.637133	-0.047232	4.119801
229.953724	5784.933374	15.642138	-0.047232	4.117065
229.964941	5776.903156	15.647143	-0.047229	4.114317
230.124326	5768.868164	15.652147	-0.047253	4.111566
229.790199	5760.844446	15.657152	-0.047186	4.108812
229.770763	5752.874321	15.662157	-0.047178	4.106078
229.829534	5744.872879	15.667162	-0.047184	4.103332
229.652049	5736.885868	15.672167	-0.047146	4.100587
229.673989	5728.935620	15.677171	-0.047145	4.097855
229.478290	5720.928348	15.682176	-0.047103	4.095098
229.590806	5712.938094	15.687181	-0.047119	4.092350
229.420253	5704.887249	15.692186	-0.047082	4.089575
229.402234	5696.893888	15.697191	-0.047074	4.086820
229.561358	5688.903435	15.702195	-0.047099	4.084067
229.375933	5680.954646	15.707200	-0.047059	4.081322
229.460028	5672.963446	15.712205	-0.047070	4.078563
229.433941	5664.962184	15.717210	-0.047060	4.075798
229.279336	5656.935462	15.722215	-0.047026	4.073021
229.302235	5648.913392	15.727219	-0.047026	4.070245
229.256273	5640.954582	15.732224	-0.047012	4.067489
229.328364	5632.919792	15.737229	-0.047021	4.064706
229.039161	5624.972871	15.742234	-0.046962	4.061946
229.154832	5616.912180	15.747239	-0.046978	4.059151
229.188316	5608.964686	15.752243	-0.046980	4.056392
228.870377	5600.926785	15.757248	-0.046915	4.053595
228.936428	5592.941293	15.762253	-0.046923	4.050819
228.911394	5584.908581	15.767258	-0.046913	4.048024
228.879557	5576.911303	15.772263	-0.046902	4.045239
228.828721	5568.975003	15.777267	-0.046888	4.042474
228.651174	5560.938578	15.782272	-0.046850	4.039669
228.871096	5552.995411	15.787277	-0.046886	4.036901
228.676066	5544.931581	15.792282	-0.046844	4.034083
228.503387	5536.814444	15.797287	-0.046807	4.031244
228.541006	5528.868020	15.802291	-0.046809	4.028467
228.668194	5520.840192	15.807296	-0.046828	4.025660
228.593896	5512.938190	15.812301	-0.046809	4.022892
228.371208	5504.902115	15.817306	-0.046763	4.020074
228.540149	5496.936328	15.822311	-0.046789	4.017284
228.566903	5488.912950	15.827315	-0.046789	4.014469
228.466511	5480.883985	15.832320	-0.046765	4.011649
228.472209	5472.911030	15.837325	-0.046762	4.008848
228.100999	5464.935781	15.842330	-0.046687	4.006038
228.340717	5456.905821	15.847335	-0.046727	4.003216
228.438215	5448.947282	15.852339	-0.046740	4.000416
228.149776	5440.954319	15.857344	-0.046682	3.997595
228.108693	5432.948706	15.862349	-0.046669	3.994772
227.978886	5424.895366	15.867354	-0.046640	3.991928
228.109472	5416.892359	15.872359	-0.046659	3.989105
228.258024	5408.898553	15.877363	-0.046682	3.986283
228.115681	5400.893899	15.882368	-0.046650	3.983450
228.250984	5392.927877	15.887373	-0.046671	3.980634
228.248576	5384.943065	15.892378	-0.046665	3.977807
227.989660	5376.950499	15.897383	-0.046612	3.974970
227.854059	5368.920945	15.902387	-0.046582	3.972121
228.062744	5360.879957	15.907392	-0.046616	3.969271
228.043981	5352.964508	15.912397	-0.046607	3.966460
227.828085	5344.964019	15.917402	-0.046562	3.963613
227.727624	5336.976981	15.922407	-0.046538	3.960772
227.771729	5329.011536	15.927411	-0.046542	3.957938
227.781951	5321.003476	15.932416	-0.046538	3.955086
227.548900	5312.934235	15.937421	-0.046490	3.952206
227.420716	5304.941107	15.942426	-0.046461	3.949353
227.463266	5296.970787	15.947431	-0.046464	3.946510
227.442207	5288.992734	15.952435	-0.046455	3.943660
227.436459	5280.951598	15.957440	-0.046449	3.940786
227.491921	5272.997059	15.962445	-0.046455	3.937942
227.403722	5264.987409	15.967450	-0.046433	3.935073
227.497733	5256.984971	15.972455	-0.046446	3.932208
227.342130	5248.973894	15.977459	-0.046412	3.929334
227.099023	5240.993178	15.982464	-0.046361	3.926467
227.203645	5233.012952	15.987469	-0.046376	3.923604
227.143376	5225.002595	15.992474	-0.046360	3.920725
226.943484	5217.010491	15.997479	-0.046318	3.917848
226.940259	5209.019473	16.002483	-0.046312	3.914973
226.972161	5200.962316	16.007488	-0.046313	3.912073
227.166746	5192.952963	16.012493	-0.046344	3.909190
226.790846	5184.992859	16.017498	-0.046269	3.906313
226.839395	5177.000270	16.022503	-0.046273	3.903430
226.932826	5169.028514	16.027507	-0.046286	3.900553
226.642033	5161.011929	16.032512	-0.046227	3.897651
226.794428	5152.997979	16.037517	-0.046250	3.894755
226.585671	5144.978819	16.042522	-0.046206	3.891849
226.614113	5136.974715	16.047527	-0.046206	3.888950
226.569122	5129.000281	16.052531	-0.046193	3.886059
226.435535	5120.986636	16.057536	-0.046163	3.883150
226.560978	5113.015907	16.062541	-0.046182	3.880259
226.518006	5105.033494	16.067546	-0.046169	3.877358
226.509740	5097.015718	16.072551	-0.046162	3.874443
226.431414	5088.767606	16.077555	-0.046142	3.871441
226.284527	5080.826217	16.082560	-0.046110	3.868546
226.356065	5072.896912	16.087565	-0.046118	3.865658
226.212694	5064.969010	16.092570	-0.046087	3.862765
226.062586	5056.982493	16.097575	-0.046054	3.859847
226.079815	5048.978334	16.102579	-0.046052	3.856924
225.984589	5040.970238	16.107584	-0.046029	3.853996
226.142929	5032.994303	16.112589	-0.046054	3.851081
225.966430	5024.957736	16.117594	-0.046016	3.848136
225.961395	5016.974899	16.122599	-0.046010	3.845212
226.166698	5009.084244	16.127603	-0.046043	3.842323
225.889475	5001.045411	16.132608	-0.045987	3.839368
225.993952	4993.099284	16.137613	-0.046001	3.836453
225.696914	4985.025634	16.142618	-0.045941	3.833480
225.820365	4977.010002	16.147623	-0.045959	3.830535
225.558447	4969.052156	16.152627	-0.045905	3.827601
225.441996	4961.015094	16.157632	-0.045879	3.824639
225.455770	4953.085211	16.162637	-0.045876	3.821716
225.594722	4945.064499	16.167642	-0.045897	3.818761
225.553278	4937.087427	16.172647	-0.045884	3.815815
225.703600	4929.074156	16.177651	-0.045907	3.812858
225.378703	4921.063478	16.182656	-0.045842	3.809889
225.267855	4913.094762	16.187661	-0.045816	3.806938
225.399839	4905.066640	16.192666	-0.045836	3.803968
225.182884	4897.114095	16.197671	-0.045791	3.801016
225.227263	4889.115388	16.202675	-0.045794	3.798051
225.279408	4881.105639	16.207680	-0.045799	3.795079
225.340415	4873.078938	16.212685	-0.045805	3.792099
225.223012	4865.037256	16.217690	-0.045778	3.789107
225.060670	4857.080160	16.222695	-0.045743	3.786143
225.070362	4849.088883	16.227699	-0.045740	3.783167
225.153249	4841.083580	16.232704	-0.045750	3.780186
224.894758	4833.126920	16.237709	-0.045697	3.777213
224.808376	4825.106856	16.242714	-0.045676	3.774218
224.924619	4817.062516	16.247719	-0.045693	3.771216
224.828549	4809.115945	16.252723	-0.045670	3.768243
224.602408	4801.078539	16.257728	-0.045623	3.765231
224.590929	4793.140360	16.262733	-0.045616	3.762258
224.445133	4785.126782	16.267738	-0.045583	3.759252
224.410273	4777.146956	16.272743	-0.045572	3.756259
224.496871	4769.121927	16.277747	-0.045583	3.753249
224.406606	4761.081051	16.282752	-0.045561	3.750226
224.343399	4753.108939	16.287757	-0.045545	3.747228
224.539240	4745.077289	16.292762	-0.045576	3.744211
224.421648	4737.149583	16.297767	-0.045549	3.741223
224.176520	4729.170031	16.302771	-0.045499	3.738210
224.008318	4721.143354	16.307776	-0.045462	3.735179
224.371274	4713.112829	16.312781	-0.045525	3.732157
224.322558	4705.087510	16.317786	-0.045511	3.729124
224.129940	4697.157973	16.322791	-0.045470	3.726122
224.121370	4689.159661	16.327795	-0.045463	3.723095
224.073098	4681.172052	16.332800	-0.045449	3.720069
224.048804	4673.205075	16.337805	-0.045440	3.717050
223.973764	4665.170516	16.342810	-0.045421	3.714000
224.015364	4657.089844	16.347815	-0.045424	3.710934
223.767374	4649.156993	16.352819	-0.045373	3.707914
223.646703	4641.113287	16.357824	-0.045345	3.704852
223.824741	4633.175728	16.362829	-0.045373	3.701836
223.701846	4625.206060	16.367834	-0.045345	3.698798
223.729736	4617.217560	16.372839	-0.045346	3.695754
223.846926	4609.209311	16.377843	-0.045363	3.692702
223.669896	4601.167374	16.382848	-0.045325	3.689627
223.691529	4593.237503	16.387853	-0.045324	3.686597
223.552035	4585.242418	16.392858	-0.045293	3.683536
223.557352	4577.250935	16.397863	-0.045289	3.680477
223.366900	4569.256351	16.402867	-0.045248	3.677410
223.166293	4561.236648	16.407872	-0.045206	3.674330
223.337126	4553.216727	16.412877	-0.045233	3.671257
223.442219	4545.229004	16.417882	-0.045247	3.668192
223.246936	4537.222723	16.422887	-0.045206	3.665110
223.278887	4529.263863	16.427891	-0.045207	3.662049
223.204261	4521.208648	16.432896	-0.045188	3.658946
223.116132	4513.283514	16.437901	-0.045167	3.655890
223.072304	4505.246314	16.442906	-0.045154	3.652789
223.100134	4497.215100	16.447911	-0.045154	3.649690
223.163744	4489.268217	16.452915	-0.045161	3.646622
222.925995	4481.276107	16.457920	-0.045111	3.643525
222.992619	4473.298919	16.462925	-0.045119	3.640440
223.130644	4465.296130	16.467930	-0.045140	3.637344
222.994195	4457.269242	16.472935	-0.045109	3.634229
223.019680	4449.249288	16.477939	-0.045109	3.631118
222.873919	4441.240925	16.482944	-0.045077	3.628005
222.858451	4433.274549	16.487949	-0.045069	3.624908
222.777364	4425.298738	16.492954	-0.045049	3.621804
222.762505	4417.308312	16.497959	-0.045041	3.618693
222.548576	4409.359646	16.502963	-0.044996	3.615590
222.360650	4401.309635	16.507968	-0.044956	3.612445
222.718563	4393.290342	16.512973	-0.045018	3.609325
222.646040	4385.322843	16.517978	-0.045000	3.606211
222.387432	4377.354792	16.522983	-0.044946	3.603088
222.589002	4369.348082	16.527987	-0.044979	3.599960
222.354790	4361.385886	16.532992	-0.044930	3.596835
222.367392	4353.356444	16.537997	-0.044928	3.593688
222.343382	4345.353380	16.543002	-0.044918	3.590547
222.278079	4337.373829	16.548007	-0.044901	3.587412
222.449760	4329.358696	16.553011	-0.044928	3.584266
222.171626	4321.422899	16.558016	-0.044871	3.581137
222.384662	4313.403671	16.563021	-0.044906	3.577985
222.030437	4305.418633	16.568026	-0.044835	3.574828
222.039472	4297.405485	16.573031	-0.044832	3.571668
222.044227	4289.425040	16.578035	-0.044828	3.568517
221.855735	4281.416919	16.583040	-0.044788	3.565348
221.851967	4273.453651	16.588045	-0.044782	3.562198
221.796062	4265.439016	16.593050	-0.044767	3.559024
221.739069	4257.465510	16.598055	-0.044751	3.555863
221.770696	4249.382354	16.603059	-0.044752	3.552659
221.451421	4241.329534	16.608064	-0.044687	3.549453
221.654385	4233.366019	16.613069	-0.044720	3.546296
221.699124	4225.391561	16.618074	-0.044724	3.543126
221.627716	4217.404732	16.623079	-0.044705	3.539945
221.607639	4209.445533	16.628083	-0.044697	3.536774
221.604254	4201.417868	16.633088	-0.044691	3.533574
221.520806	4193.412936	16.638093	-0.044671	3.530377
221.591504	4185.439521	16.643098	-0.044679	3.527194
221.640139	4177.429684	16.648103	-0.044683	3.523994
221.271614	4169.540858	16.653107	-0.044609	3.520826
221.139928	4161.507931	16.658112	-0.044580	3.517604
221.215223	4153.500788	16.663117	-0.044589	3.514397
221.231544	4145.486799	16.668122	-0.044587	3.511182
221.044621	4137.516809	16.673127	-0.044547	3.507975
221.095867	4129.494630	16.678131	-0.044552	3.504752
221.089302	4121.544790	16.683136	-0.044545	3.501553
221.108309	4113.556842	16.688141	-0.044544	3.498337
220.857903	4105.550784	16.693146	-0.044492	3.495102
220.944401	4097.516654	16.698151	-0.044503	3.491863
221.154455	4089.578401	16.703155	-0.044538	3.488664
220.796015	4081.577717	16.708160	-0.044466	3.485419
220.771476	4073.590766	16.713165	-0.044456	3.482187
220.525906	4065.640246	16.718170	-0.044406	3.478959
220.617531	4057.615891	16.723175	-0.044418	3.475709
220.556084	4049.582683	16.728179	-0.044401	3.472448
220.481691	4041.558084	16.733184	-0.044383	3.469187
220.489594	4033.583644	16.738189	-0.044379	3.465946
220.327841	4025.623312	16.743194	-0.044344	3.462702
220.330778	4017.600632	16.748199	-0.044339	3.459434
220.337324	4009.662561	16.753203	-0.044336	3.456199
220.163247	4001.630208	16.758208	-0.044298	3.452916
220.176138	3993.608076	16.763213	-0.044296	3.449640
220.107155	3985.624607	16.768218	-0.044278	3.446374
220.112185	3977.632831	16.773223	-0.044274	3.443104
220.223095	3969.675096	16.778227	-0.044290	3.439848
220.328066	3961.677379	16.783232	-0.044304	3.436573
220.166379	3953.675545	16.788237	-0.044269	3.433284
220.077047	3945.645151	16.793242	-0.044247	3.429982
219.970796	3937.658076	16.798247	-0.044223	3.426695
220.297063	3929.683358	16.803251	-0.044278	3.423424
219.880996	3921.717425	16.808256	-0.044196	3.420128
219.831192	3913.770747	16.813261	-0.044182	3.416850
219.885113	3905.702928	16.818266	-0.044187	3.413522
219.895709	3897.707730	16.823271	-0.044184	3.410219
219.788841	3889.754945	16.828275	-0.044159	3.406927
219.615455	3881.727247	16.833280	-0.044122	3.403598
219.775783	3873.774499	16.838285	-0.044147	3.400308
219.591581	3865.813084	16.843290	-0.044107	3.397000
219.506959	3857.784263	16.848295	-0.044087	3.393663
219.443755	3849.706765	16.853299	-0.044070	3.390304
219.481210	3841.717335	16.858304	-0.044072	3.386982
219.641673	3833.748566	16.863309	-0.044097	3.383670
219.622102	3825.772084	16.868314	-0.044088	3.380345
219.608112	3817.825427	16.873319	-0.044081	3.377029
219.555877	3809.832306	16.878323	-0.044066	3.373689
219.546747	3801.791948	16.883328	-0.044059	3.370327
219.291933	3793.855189	16.888333	-0.044007	3.366997
219.197621	3785.855295	16.893338	-0.043984	3.363643
219.120493	3777.863442	16.898343	-0.043965	3.360289
219.158510	3769.893491	16.903347	-0.043967	3.356946
218.948192	3761.886038	16.908352	-0.043923	3.353574
218.921740	3753.869365	16.913357	-0.043913	3.350201
219.007547	3745.860691	16.918362	-0.043924	3.346833
218.970926	3737.875116	16.923367	-0.043912	3.343467
219.074385	3729.905388	16.928371	-0.043926	3.340109
218.733218	3721.939544	16.933376	-0.043858	3.336732
218.713990	3713.932381	16.938381	-0.043849	3.333347
218.812999	3705.901620	16.943386	-0.043863	3.329953
218.685868	3697.944534	16.948391	-0.043834	3.326578
218.793467	3689.944760	16.953395	-0.043849	3.323190
218.628038	3681.963936	16.958400	-0.043813	3.319797
218.478873	3674.014889	16.963405	-0.043781	3.316414
218.484256	3665.997240	16.968410	-0.043777	3.313005
218.587090	3657.944014	16.973415	-0.043791	3.309580
218.646404	3649.989349	16.978419	-0.043797	3.306193
218.506840	3641.991784	16.983424	-0.043766	3.302776
218.413528	3634.043006	16.988429	-0.043744	3.299378
218.438507	3626.062678	16.993434	-0.043743	3.295967
218.213085	3618.044524	16.998439	-0.043696	3.292527
218.406442	3610.056208	17.003443	-0.043727	3.289113
218.358257	3602.051293	17.008448	-0.043713	3.285678
218.110986	3594.107644	17.013453	-0.043662	3.282259
218.078975	3586.115156	17.018458	-0.043652	3.278823
218.067536	3578.120494	17.023463	-0.043644	3.275384
218.151372	3570.106015	17.028467	-0.043655	3.271936
217.907239	3562.096521	17.033472	-0.043605	3.268473
217.967027	3554.111281	17.038477	-0.043611	3.265030
217.924997	3546.151697	17.043482	-0.043598	3.261590
217.861157	3538.158519	17.048487	-0.043581	3.258130
217.886942	3530.180048	17.053491	-0.043581	3.254677
217.901563	3522.157782	17.058496	-0.043579	3.251201
217.696808	3514.185183	17.063501	-0.043536	3.247734
217.700194	3506.176815	17.068506	-0.043531	3.244257
217.583142	3498.244172	17.073511	-0.043505	3.240803
217.607529	3490.276089	17.078515	-0.043504	3.237336
217.452685	3482.250129	17.083520	-0.043470	3.233833
217.454242	3474.180454	17.088525	-0.043466	3.230313
217.314228	3466.221407	17.093530	-0.043435	3.226832
217.302731	3458.206170	17.098535	-0.043427	3.223328
217.396877	3450.247506	17.103539	-0.043440	3.219849
217.393576	3442.263110	17.108544	-0.043434	3.216351
217.194586	3434.290178	17.113549	-0.043392	3.212846
217.149297	3426.288801	17.118554	-0.043379	3.209332
217.163090	3418.293468	17.123559	-0.043377	3.205818
217.105351	3410.338493	17.128563	-0.043361	3.202316
216.943903	3402.343304	17.133568	-0.043326	3.198787
216.814535	3394.381563	17.138573	-0.043297	3.195271
216.817640	3386.355947	17.143578	-0.043292	3.191728
216.772238	3378.349524	17.148583	-0.043279	3.188188
216.777699	3370.376771	17.153587	-0.043275	3.184660
216.822495	3362.408374	17.158592	-0.043278	3.181133
216.692461	3354.427599	17.163597	-0.043249	3.177588
216.891614	3346.400200	17.168602	-0.043281	3.174033
216.727579	3338.410422	17.173607	-0.043246	3.170476
216.665299	3330.420559	17.178611	-0.043229	3.166918
216.552115	3322.446041	17.183616	-0.043203	3.163361
216.750005	3314.472747	17.188621	-0.043235	3.159814
216.817198	3306.504947	17.193626	-0.043243	3.156260
216.717799	3298.476452	17.198631	-0.043219	3.152668
216.673478	3290.475493	17.203635	-0.043206	3.149086
216.731729	3282.465267	17.208640	-0.043212	3.145500
216.607663	3274.538377	17.213645	-0.043184	3.141940
216.240528	3266.604101	17.218650	-0.043110	3.138361
216.358808	3258.568814	17.223655	-0.043127	3.134755
216.450706	3250.586228	17.228659	-0.043139	3.131167
216.164665	3242.589142	17.233664	-0.043081	3.127551
216.319337	3234.620773	17.238669	-0.043105	3.123964
216.244058	3226.654578	17.243674	-0.043086	3.120363
216.094047	3218.647759	17.248679	-0.043053	3.116737
216.000381	3210.680574	17.253683	-0.043031	3.113126
216.089037	3202.628750	17.258688	-0.043042	3.109482
216.104829	3194.645875	17.263693	-0.043040	3.105861
215.768575	3186.706188	17.268698	-0.042973	3.102239
216.013436	3178.681266	17.273703	-0.043013	3.098601
215.977881	3170.720568	17.278707	-0.043002	3.094975
215.671273	3162.723962	17.283712	-0.042940	3.091316
215.896961	3154.720181	17.288717	-0.042977	3.087674
215.897920	3146.738894	17.293722	-0.042972	3.084028
215.566562	3138.800031	17.298727	-0.042905	3.080381
215.425352	3130.845990	17.303731	-0.042874	3.076732
215.492197	3122.797963	17.308736	-0.042881	3.073045
215.657166	3114.739371	17.313741	-0.042907	3.069353
215.478872	3106.781776	17.318746	-0.042869	3.065687
215.245465	3098.821800	17.323751	-0.042821	3.062013
215.497276	3090.824487	17.328755	-0.042862	3.058340
215.161186	3082.860484	17.333760	-0.042795	3.054651
215.144440	3074.870052	17.338765	-0.042787	3.050960
215.114545	3066.894028	17.343770	-0.042776	3.047270
215.015406	3058.918656	17.348775	-0.042753	3.043573
214.910522	3050.975160	17.353779	-0.042728	3.039886
214.888587	3042.993097	17.358784	-0.042719	3.036180
215.219160	3034.940549	17.363789	-0.042776	3.032455
215.057912	3026.948212	17.368794	-0.042741	3.028728
214.745054	3018.985613	17.373799	-0.042678	3.025004
214.872882	3011.044508	17.378803	-0.042697	3.021307
214.719229	3003.030249	17.383808	-0.042663	3.017557
214.732223	2995.038600	17.388813	-0.042660	3.013821
214.851916	2987.018993	17.393818	-0.042678	3.010073
214.674822	2979.047850	17.398823	-0.042640	3.006328
214.709424	2971.087697	17.403827	-0.042641	3.002594
214.702463	2963.108615	17.408832	-0.042635	2.998845
214.659296	2955.144672	17.413837	-0.042622	2.995096
214.444000	2947.144712	17.418842	-0.042577	2.991317
214.201491	2939.150587	17.423847	-0.042527	2.987534
214.319227	2931.166067	17.428851	-0.042544	2.983769
214.122525	2923.213182	17.433856	-0.042502	2.979999
214.245520	2915.223169	17.438861	-0.042520	2.976222
214.255961	2907.212489	17.443866	-0.042517	2.972425
214.330127	2899.213759	17.448871	-0.042526	2.968632
214.254517	2891.237345	17.453875	-0.042507	2.964837
214.035209	2883.298429	17.458880	-0.042461	2.961048
214.149007	2875.316245	17.463885	-0.042477	2.957251
214.070375	2867.342778	17.468890	-0.042458	2.953442
214.004110	2859.301237	17.473895	-0.042440	2.949597
214.122968	2851.318008	17.478899	-0.042457	2.945785
214.144100	2843.336761	17.483904	-0.042456	2.941963
213.930664	2835.389405	17.488909	-0.042412	2.938140
213.844407	2827.415925	17.493914	-0.042391	2.934307
213.803693	2819.417449	17.498919	-0.042378	2.930459
213.863006	2811.440609	17.503923	-0.042384	2.926621
213.737066	2803.457582	17.508928	-0.042356	2.922766
213.752181	2795.481328	17.513933	-0.042354	2.918916
213.861075	2787.515619	17.518938	-0.042369	2.915071
213.534123	2779.455539	17.523943	-0.042303	2.911153
213.641853	2771.470594	17.528947	-0.042318	2.907288
213.445134	2763.515027	17.533952	-0.042277	2.903417
213.259023	2755.545251	17.538957	-0.042237	2.899533
213.131912	2747.604718	17.543962	-0.042208	2.895662
213.093432	2739.596531	17.548967	-0.042196	2.891758
213.176615	2731.618904	17.553971	-0.042207	2.887870
213.049204	2723.629451	17.558976	-0.042178	2.883959
213.121894	2715.670670	17.563981	-0.042187	2.880069
213.044653	2707.703693	17.568986	-0.042167	2.876162
212.903174	2699.699449	17.573991	-0.042136	2.872227
213.110194	2691.714805	17.578995	-0.042170	2.868316
213.067663	2683.718867	17.584000	-0.042157	2.864380
212.831363	2675.791839	17.589005	-0.042108	2.860462
212.727573	2667.827979	17.594010	-0.042083	2.856528
212.648983	2659.819882	17.599015	-0.042064	2.852567
212.757614	2651.816915	17.604019	-0.042079	2.848614
212.457727	2643.861192	17.609024	-0.042018	2.844657
212.595233	2635.909212	17.614029	-0.042039	2.840720
212.463175	2627.930361	17.619034	-0.042009	2.836749
212.461582	2619.914660	17.624039	-0.042004	2.832762
212.489275	2611.915047	17.629043	-0.042004	2.828778
212.421695	2603.905049	17.634048	-0.041987	2.824779
212.358268	2595.980897	17.639053	-0.041970	2.820816
212.166322	2588.038988	17.644058	-0.041929	2.816832
212.179474	2580.016993	17.649063	-0.041927	2.812814
212.209498	2572.010107	17.654067	-0.041927	2.808799
212.128129	2564.032454	17.659072	-0.041907	2.804787
212.319589	2556.085004	17.664077	-0.041938	2.800799
212.146015	2548.133372	17.669082	-0.041901	2.796783
211.888259	2540.161578	17.674087	-0.041848	2.792745
212.006767	2532.143619	17.679091	-0.041865	2.788701
211.833736	2524.156910	17.684096	-0.041828	2.784649
211.777598	2516.231110	17.689101	-0.041812	2.780629
211.747342	2508.268295	17.694106	-0.041802	2.776586
211.598788	2500.249269	17.699111	-0.041769	2.772502
211.817016	2492.258702	17.704115	-0.041805	2.768447
211.704390	2484.274405	17.709120	-0.041779	2.764371
211.654940	2476.346478	17.714125	-0.041764	2.760320
211.899108	2468.354826	17.719130	-0.041805	2.756249
211.596016	2460.319228	17.724135	-0.041744	2.752117
211.705753	2452.314725	17.729139	-0.041759	2.748019
211.490405	2444.344694	17.734144	-0.041714	2.743913
211.501970	2436.409609	17.739149	-0.041711	2.739832
211.327385	2428.477502	17.744154	-0.041674	2.735736
211.291546	2420.455640	17.749159	-0.041662	2.731596
211.362074	2412.485847	17.754163	-0.041670	2.727482
211.114914	2404.525462	17.759168	-0.041619	2.723348
211.190291	2396.562317	17.764173	-0.041628	2.719226
210.998056	2388.628138	17.769178	-0.041588	2.715096
210.971250	2380.600526	17.774183	-0.041578	2.710922
210.993492	2372.623756	17.779187	-0.041577	2.706771
211.225398	2364.625071	17.784192	-0.041615	2.702615
211.308848	2356.683282	17.789197	-0.041626	2.698473
211.053291	2348.719298	17.794202	-0.041573	2.694291
211.047182	2340.713918	17.799207	-0.041567	2.690098
211.033542	2332.771878	17.804211	-0.041559	2.685930
210.883483	2324.786244	17.809216	-0.041526	2.681724
210.989908	2316.837267	17.814221	-0.041541	2.677548
210.718995	2308.874222	17.819226	-0.041486	2.673333
210.627964	2300.857707	17.824231	-0.041464	2.669095
210.536285	2292.884139	17.829235	-0.041442	2.664873
210.778420	2284.912000	17.834240	-0.041482	2.660666
210.451337	2276.964218	17.839245	-0.041416	2.656429
210.267675	2268.998254	17.844250	-0.041377	2.652185
210.227610	2260.986225	17.849255	-0.041365	2.647918
210.375374	2253.030503	17.854259	-0.041387	2.643687
210.355997	2245.058305	17.859264	-0.041379	2.639430
210.319597	2237.122074	17.864269	-0.041367	2.635184
210.323529	2229.122043	17.869274	-0.041363	2.630899
210.309337	2221.128263	17.874279	-0.041355	2.626609
210.161687	2213.202945	17.879283	-0.041323	2.622341
210.027553	2205.233012	17.884288	-0.041293	2.618042
210.045505	2197.262004	17.889293	-0.041291	2.613746
209.908364	2189.268193	17.894298	-0.041261	2.609420
210.071913	2181.278552	17.899303	-0.041286	2.605109
210.093331	2173.342778	17.904307	-0.041285	2.600811
209.877214	2165.390268	17.909312	-0.041240	2.596481
209.962028	2157.298478	17.914317	-0.041251	2.592087
209.645309	2149.301275	17.919322	-0.041187	2.587711
209.519382	2141.344754	17.924327	-0.041158	2.583362
209.496803	2133.434104	17.929331	-0.041149	2.579039
209.451959	2125.462589	17.934336	-0.041136	2.574673
209.491637	2117.496812	17.939341	-0.041138	2.570308
209.388074	2109.535346	17.944346	-0.041114	2.565929
209.339439	2101.591645	17.949351	-0.041100	2.561556
209.422525	2093.634107	17.954355	-0.041111	2.557176
209.331900	2085.651417	17.959360	-0.041089	2.552764
209.308392	2077.669547	17.964365	-0.041079	2.548348
209.236023	2069.717585	17.969370	-0.041061	2.543938
209.170507	2061.769301	17.974375	-0.041044	2.539523
209.175899	2053.831161	17.979379	-0.041040	2.535111
208.963654	2045.835475	17.984384	-0.040995	2.530644
208.930879	2037.866583	17.989389	-0.040984	2.526197
208.991397	2029.904811	17.994394	-0.040991	2.521752
208.987593	2021.959434	17.999399	-0.040985	2.517304
208.813347	2014.012728	18.004403	-0.040948	2.512835
208.647979	2005.992223	18.009408	-0.040912	2.508318
208.693947	1998.018328	18.014413	-0.040915	2.503833
208.761571	1990.054782	18.019418	-0.040923	2.499348
208.588183	1982.117583	18.024423	-0.040886	2.494853
208.825486	1974.118748	18.029427	-0.040925	2.490344
208.602896	1966.170758	18.034432	-0.040879	2.485822
208.707494	1958.205040	18.039437	-0.040893	2.481306
208.592582	1950.267218	18.044442	-0.040867	2.476782
208.500969	1942.300982	18.049447	-0.040845	2.472234
208.547545	1934.336893	18.054451	-0.040848	2.467690
208.418785	1926.377352	18.059456	-0.040820	2.463127
208.311331	1918.430935	18.064461	-0.040795	2.458565
208.300554	1910.468196	18.069466	-0.040788	2.453991
208.260591	1902.479399	18.074471	-0.040775	2.449393
208.190816	1894.542549	18.079475	-0.040757	2.444813
207.848670	1886.609450	18.084480	-0.040689	2.440206
207.750248	1878.661315	18.089485	-0.040665	2.435600
207.786504	1870.617679	18.094490	-0.040667	2.430940
207.859245	1862.618177	18.099495	-0.040676	2.426300
207.817032	1854.684781	18.104499	-0.040663	2.421680
207.693920	1846.732055	18.109504	-0.040635	2.417035
207.548690	1838.796290	18.114509	-0.040603	2.412388
207.627900	1830.812226	18.119514	-0.040613	2.407721
207.577116	1822.842533	18.124519	-0.040598	2.403044
207.657815	1814.908543	18.129523	-0.040608	2.398389
207.540661	1806.960146	18.134528	-0.040582	2.393701
207.451401	1798.980298	18.139533	-0.040560	2.388987
207.296162	1791.033788	18.144538	-0.040526	2.384279
207.317703	1783.088846	18.149543	-0.040525	2.379576
207.531225	1775.121721	18.154547	-0.040560	2.374866
207.317001	1767.160091	18.159552	-0.040515	2.370115
207.200955	1759.217041	18.164557	-0.040489	2.365374
207.192260	1751.269496	18.169562	-0.040482	2.360629
206.939153	1743.350332	18.174567	-0.040430	2.355872
206.894589	1735.362397	18.179571	-0.040417	2.351081
206.762680	1727.393243	18.184576	-0.040387	2.346285
206.821791	1719.421812	18.189581	-0.040393	2.341492
206.790529	1711.480734	18.194586	-0.040383	2.336701
206.729412	1703.506593	18.199591	-0.040366	2.331878
206.816728	1695.549626	18.204595	-0.040378	2.327067
206.547551	1687.629391	18.209600	-0.040323	2.322239
206.540081	1679.680052	18.214605	-0.040316	2.317405
206.420059	1671.750145	18.219610	-0.040289	2.312563
206.471225	1663.747071	18.224615	-0.040293	2.307681
206.488232	1655.810168	18.229619	-0.040292	2.302826
206.268818	1647.879217	18.234624	-0.040246	2.297944
206.322969	1639.910121	18.239629	-0.040251	2.293052
206.265276	1631.957181	18.244634	-0.040235	2.288149
206.205962	1624.010416	18.249639	-0.040219	2.283240
206.102634	1616.086596	18.254643	-0.040195	2.278331
206.092557	1608.099592	18.259648	-0.040188	2.273380
206.083020	1600.081960	18.264653	-0.040182	2.268399
205.839827	1592.167186	18.269658	-0.040131	2.263451
205.854546	1584.217808	18.274663	-0.040129	2.258492
206.003917	1576.263146	18.279667	-0.040152	2.253532
205.960171	1568.292312	18.284672	-0.040139	2.248533
205.784301	1560.383214	18.289677	-0.040101	2.243551
205.905360	1552.437200	18.294682	-0.040119	2.238560
205.820948	1544.490825	18.299687	-0.040098	2.233539
205.822713	1536.533770	18.304691	-0.040093	2.228509
205.550932	1528.616536	18.309696	-0.040038	2.223467
205.607348	1520.666687	18.314701	-0.040044	2.218423
205.567251	1512.723696	18.319706	-0.040031	2.213363
205.508571	1504.749447	18.324711	-0.040015	2.208270
205.712799	1496.806534	18.329715	-0.040048	2.203209
205.234777	1488.921840	18.334720	-0.039954	2.198111
205.268915	1480.963214	18.339725	-0.039956	2.193001
205.280617	1472.985357	18.344730	-0.039953	2.187864
205.153839	1465.035937	18.349735	-0.039924	2.182721
205.036698	1457.128779	18.354739	-0.039898	2.177594
205.101993	1449.149470	18.359744	-0.039905	2.172425
205.105944	1441.196620	18.364749	-0.039901	2.167255
204.779257	1433.315351	18.369754	-0.039835	2.162089
204.944100	1425.345280	18.374759	-0.039861	2.156898
205.086304	1417.391063	18.379763	-0.039882	2.151703
204.920727	1409.445347	18.384768	-0.039846	2.146472
204.943570	1401.510111	18.389773	-0.039846	2.141253
204.989829	1393.576645	18.394778	-0.039849	2.136024
204.763876	1385.646487	18.399783	-0.039802	2.130759
204.620729	1377.733102	18.404787	-0.039771	2.125500
204.596089	1369.789940	18.409792	-0.039761	2.120219
204.651002	1361.854153	18.414797	-0.039767	2.114938
204.370236	1353.869428	18.419802	-0.039709	2.109578
204.338319	1345.924608	18.424807	-0.039698	2.104256
204.371828	1338.011088	18.429811	-0.039700	2.098947
204.141312	1330.097218	18.434816	-0.039652	2.093599
204.189167	1322.138114	18.439821	-0.039656	2.088234
204.088593	1314.220758	18.444826	-0.039632	2.082868
203.840530	1306.320041	18.449831	-0.039581	2.077486
203.910462	1298.385584	18.454835	-0.039589	2.072098
203.929644	1290.414836	18.459840	-0.039588	2.066666
203.903056	1282.489714	18.464845	-0.039578	2.061247
203.543562	1274.625282	18.469850	-0.039506	2.055821
203.574286	1266.642777	18.474855	-0.039507	2.050339
203.747241	1258.697809	18.479859	-0.039534	2.044883
203.592181	1250.786204	18.484864	-0.039500	2.039402
203.495875	1242.880793	18.489869	-0.039477	2.033916
203.435920	1234.919135	18.494874	-0.039461	2.028380
203.270979	1227.000986	18.499879	-0.039426	2.022848
203.328197	1219.080270	18.504883	-0.039431	2.017323
203.329635	1211.126883	18.509888	-0.039427	2.011753
203.383947	1203.190326	18.514893	-0.039432	2.006186
203.215913	1195.306486	18.519898	-0.039396	2.000617
203.130325	1187.392951	18.524903	-0.039375	1.995019
203.190747	1179.447382	18.529907	-0.039381	1.989399
203.120888	1171.523168	18.534912	-0.039363	1.983764
202.979713	1163.626434	18.539917	-0.039332	1.978126
203.276272	1155.666464	18.544922	-0.039382	1.972472
203.166257	1147.744531	18.549927	-0.039357	1.966786
202.836474	1139.894503	18.554931	-0.039291	1.961112
202.971098	1131.957622	18.559936	-0.039311	1.955408
203.190041	1123.942448	18.564941	-0.039346	1.949641
203.007521	1116.054519	18.569946	-0.039308	1.943905
202.699368	1108.173714	18.574951	-0.039245	1.938143
202.811446	1100.237686	18.579955	-0.039261	1.932370
202.517048	1092.337714	18.584960	-0.039202	1.926561
202.369244	1084.456441	18.589965	-0.039169	1.920765
202.290177	1076.561964	18.594970	-0.039149	1.914949
202.288405	1068.612426	18.599975	-0.039144	1.909083
202.327573	1060.702562	18.604979	-0.039147	1.903233
202.441149	1052.765145	18.609984	-0.039163	1.897353
202.406103	1044.853642	18.614989	-0.039151	1.891457
202.322558	1036.955192	18.619994	-0.039131	1.885547
202.111158	1029.077305	18.624999	-0.039087	1.879619
202.204891	1021.169182	18.630003	-0.039099	1.873684
201.971306	1013.248762	18.635008	-0.039051	1.867684
201.912698	1005.347605	18.640013	-0.039035	1.861699
201.919766	997.443544	18.645018	-0.039031	1.855700
201.906038	989.504127	18.650023	-0.039024	1.849653
201.809522	981.632519	18.655027	-0.039001	1.843627
201.915331	973.717386	18.660032	-0.039016	1.837573
201.741037	965.840488	18.665037	-0.038978	1.831494
201.793591	957.923816	18.670042	-0.038983	1.825392
201.613184	950.045698	18.675047	-0.038945	1.819271
201.835430	942.123623	18.680051	-0.038981	1.813144
201.688839	934.232318	18.685056	-0.038949	1.806975
201.487628	926.377499	18.690061	-0.038907	1.800807
201.223368	918.527333	18.695066	-0.038852	1.794614
201.243320	910.542442	18.700071	-0.038851	1.788328
201.083297	902.667738	18.705075	-0.038817	1.782085
201.024237	894.779683	18.710080	-0.038801	1.775821
200.967553	886.878960	18.715085	-0.038785	1.769526
200.777238	879.017244	18.720090	-0.038745	1.763223
200.733063	871.139187	18.725095	-0.038732	1.756902
200.850223	863.229397	18.730099	-0.038749	1.750553
200.664193	855.352552	18.735104	-0.038709	1.744169
200.561541	847.490070	18.740109	-0.038685	1.737784
200.700857	839.567622	18.745114	-0.038706	1.731358
200.616302	831.687998	18.750119	-0.038685	1.724914
200.469037	823.865769	18.755123	-0.038653	1.718484
200.173957	816.014919	18.760128	-0.038593	1.711988
200.204852	808.095925	18.765133	-0.038594	1.705453
200.286818	800.211542	18.770138	-0.038604	1.698928
200.000609	792.359688	18.775143	-0.038546	1.692357
200.113634	784.456189	18.780147	-0.038562	1.685770
200.109349	776.588429	18.785152	-0.038557	1.679171
199.977542	768.747336	18.790157	-0.038527	1.672552
199.831595	760.881731	18.795162	-0.038495	1.665884
199.788623	753.008025	18.800167	-0.038482	1.659196
199.961206	745.120589	18.805171	-0.038510	1.652498
199.788129	737.270260	18.810176	-0.038472	1.645758
199.741829	729.434156	18.815181	-0.038459	1.639019
199.772401	721.543945	18.820186	-0.038460	1.632217
199.556913	713.662758	18.825191	-0.038415	1.625360
199.600550	705.811998	18.830195	-0.038418	1.618536
199.444381	697.974014	18.835200	-0.038384	1.611667
199.247114	690.133884	18.840205	-0.038342	1.604760
199.291693	682.294797	18.845210	-0.038346	1.597859
199.440726	674.399261	18.850215	-0.038369	1.590893
199.383244	666.569227	18.855219	-0.038353	1.583925
199.100616	658.768591	18.860224	-0.038296	1.576920
198.993250	650.928187	18.865229	-0.038271	1.569873
199.091794	643.071422	18.870234	-0.038284	1.562809
198.761117	635.282089	18.875239	-0.038218	1.555712
198.754689	627.427924	18.880243	-0.038212	1.548571
198.542739	619.594814	18.885248	-0.038167	1.541386
198.502183	611.756978	18.890253	-0.038155	1.534188
198.593309	603.904916	18.895258	-0.038167	1.526962
198.498003	596.084358	18.900263	-0.038144	1.519704
198.637027	588.252963	18.905267	-0.038165	1.512436
198.532285	580.426128	18.910272	-0.038141	1.505100
198.588322	572.610725	18.915277	-0.038147	1.497764
198.353499	564.822975	18.920282	-0.038098	1.490372
198.243718	557.010097	18.925287	-0.038073	1.482940
198.294999	549.202355	18.930291	-0.038077	1.475500
198.100224	541.353867	18.935296	-0.038036	1.467944
197.964773	533.569617	18.940301	-0.038006	1.460420
197.904113	525.779327	18.945306	-0.037990	1.452864
198.003526	517.928836	18.950311	-0.038004	1.445235
197.847223	510.188903	18.955315	-0.037970	1.437633
197.644657	502.403034	18.960320	-0.037927	1.429937
197.452814	494.626297	18.965325	-0.037887	1.422211
197.729256	486.800103	18.970330	-0.037933	1.414470
197.491509	479.028123	18.975335	-0.037884	1.406656
197.381092	471.277325	18.980339	-0.037859	1.398840
197.313072	463.486354	18.985344	-0.037841	1.390947
197.277237	455.699339	18.990349	-0.037830	1.383018
197.122288	447.950543	18.995354	-0.037796	1.375063
197.019337	440.173585	19.000359	-0.037772	1.367041
197.048656	432.416619	19.005363	-0.037773	1.359015
197.008773	424.648403	19.010368	-0.037761	1.350918
197.124817	416.866458	19.015373	-0.037777	1.342785
197.013381	409.137292	19.020378	-0.037752	1.334618
196.688253	401.420726	19.025383	-0.037686	1.326376
196.587328	393.708429	19.030387	-0.037663	1.318127
196.736551	385.833483	19.035392	-0.037686	1.309696
196.488508	378.095255	19.040397	-0.037635	1.301286
196.344239	370.401445	19.045402	-0.037603	1.292889
196.305446	362.666090	19.050407	-0.037591	1.284411
196.453338	354.935826	19.055411	-0.037614	1.275917
196.341801	347.231308	19.060416	-0.037588	1.267346
196.248749	339.545211	19.065421	-0.037566	1.258741
196.203644	331.846688	19.070426	-0.037553	1.250072
196.269805	324.129125	19.075431	-0.037560	1.241342
195.998263	316.495459	19.080435	-0.037505	1.232580
195.747532	308.814289	19.085440	-0.037454	1.223705
195.854499	301.107242	19.090445	-0.037469	1.214806
195.815241	293.429999	19.095450	-0.037457	1.205847
195.516786	285.809634	19.100455	-0.037396	1.196835
195.622038	278.124784	19.105459	-0.037411	1.187760
195.472296	270.482836	19.110464	-0.037379	1.178615
195.499187	262.820828	19.115469	-0.037379	1.169411
195.350703	255.204761	19.120474	-0.037346	1.160152
195.272983	247.550632	19.125479	-0.037327	1.150788
195.128206	239.923333	19.130483	-0.037296	1.141365
195.005676	232.313250	19.135488	-0.037268	1.131890
195.159425	224.664704	19.140493	-0.037292	1.122346
194.936127	217.110016	19.145498	-0.037246	1.112758
194.866899	209.510840	19.150503	-0.037228	1.103063
194.886724	201.925228	19.155507	-0.037227	1.093319
194.592092	194.380463	19.160512	-0.037167	1.083470
194.486998	186.830263	19.165517	-0.037143	1.073567
194.520768	179.246375	19.170522	-0.037145	1.063558
194.411098	171.708520	19.175527	-0.037120	1.053483
194.345747	164.176859	19.180531	-0.037103	1.043329
194.224080	156.668627	19.185536	-0.037075	1.033094
194.071074	149.169349	19.190541	-0.037042	1.022761
193.999145	141.679630	19.195546	-0.037024	1.012356
193.660195	134.229433	19.200551	-0.036957	1.001833
193.922218	126.690327	19.205555	-0.037001	0.991220
193.819464	119.208777	19.210560	-0.036977	0.980484
193.641896	111.777266	19.215565	-0.036939	0.969683
193.685883	104.335713	19.220570	-0.036943	0.958802
193.539557	96.922615	19.225575	-0.036911	0.947790
193.433853	89.538981	19.230579	-0.036887	0.936702
193.208733	82.175424	19.235584	-0.036840	0.925481
193.187494	74.802836	19.240589	-0.036832	0.914163
193.032575	67.457122	19.245594	-0.036798	0.902708
192.626105	60.401781	19.250599	-0.036718	0.891496