Thu Mar 11 18:50:01 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.092223	-0.069301	0.000000	-0.000063	0.725211

0.763463	-0.006722	0.005005	-0.000002	0.725219
0.936242	-0.042569	0.010010	-0.000035	0.725210
0.957801	-0.042155	0.015014	-0.000039	0.725218
0.811519	-0.017649	0.020019	-0.000012	0.725216
0.762479	-0.061940	0.025024	-0.000003	0.725113
0.941453	-0.206826	0.030029	-0.000037	0.724892
0.749163	-0.176921	0.035034	-0.000001	0.724884
0.851424	-0.189879	0.040038	-0.000021	0.724895
0.873580	-0.197074	0.045043	-0.000025	0.724889
0.809635	-0.188462	0.050048	-0.000013	0.724884
0.895840	-0.199399	0.055053	-0.000030	0.724893
0.676637	-0.165461	0.060058	0.000011	0.724884
0.961433	-0.213508	0.065062	-0.000042	0.724890
0.928726	-0.209340	0.070067	-0.000037	0.724887
0.907869	-0.205885	0.075072	-0.000033	0.724887
0.933582	-0.321777	0.080077	-0.000038	0.724670
0.761725	-0.330445	0.085082	-0.000006	0.724593
0.963858	-0.365014	0.090086	-0.000044	0.724597
0.783565	-0.333613	0.095091	-0.000011	0.724596
0.764759	-0.331082	0.100096	-0.000008	0.724595
0.652784	-0.308733	0.105101	0.000013	0.724600
0.563896	-0.382728	0.110106	0.000029	0.724425
0.740018	-0.496068	0.115110	-0.000004	0.724265
0.670944	-0.486261	0.120115	0.000009	0.724260
0.768921	-0.503803	0.125120	-0.000010	0.724261
0.839796	-0.513849	0.130125	-0.000023	0.724266
0.881641	-0.616697	0.135130	-0.000031	0.724080
0.575581	-0.624828	0.140134	0.000026	0.723958
0.763915	-0.660012	0.145139	-0.000010	0.723955
0.747146	-0.657444	0.150144	-0.000007	0.723955
0.769545	-0.720059	0.155149	-0.000011	0.723840
0.724042	-0.819526	0.160154	-0.000003	0.723630
0.957863	-0.857232	0.165158	-0.000047	0.723638
0.742019	-0.820057	0.170163	-0.000007	0.723636
0.896897	-0.959590	0.175168	-0.000036	0.723417
0.962585	-1.007377	0.180173	-0.000048	0.723347
0.858939	-0.993760	0.185178	-0.000029	0.723338
0.814501	-1.070656	0.190182	-0.000021	0.723172
0.902944	-1.170276	0.195187	-0.000038	0.723008
0.811362	-1.156496	0.200192	-0.000021	0.723004
0.827095	-1.235513	0.205197	-0.000024	0.722855
0.749922	-1.306961	0.210202	-0.000010	0.722688
0.891734	-1.327696	0.215206	-0.000037	0.722698
0.800213	-1.423254	0.220211	-0.000020	0.722479
0.717205	-1.463085	0.225216	-0.000005	0.722372
0.822730	-1.477362	0.230221	-0.000025	0.722381
0.851534	-1.638292	0.235226	-0.000030	0.722076
0.808242	-1.629093	0.240230	-0.000022	0.722079
0.649973	-1.679374	0.245235	0.000007	0.721926
0.704534	-1.782312	0.250240	-0.000004	0.721743
0.687760	-1.782205	0.255245	-0.000001	0.721738
0.566732	-1.913934	0.260250	0.000022	0.721437
0.468962	-1.894003	0.265254	0.000040	0.721443
0.245191	-1.956525	0.270259	0.000081	0.721242
-0.068180	-1.962226	0.275264	0.000139	0.721121
-0.038452	-1.982859	0.280269	0.000133	0.721092
-1.143320	-1.894300	0.285274	0.000339	0.720879
-1.793840	-1.776852	0.290278	0.000460	0.720883
-1.721758	-1.819978	0.295283	0.000446	0.720824
-3.066436	-1.725863	0.300288	0.000696	0.720539
-2.900750	-1.751423	0.305293	0.000665	0.720547
-2.958420	-1.748668	0.310298	0.000675	0.720533
-3.014103	-1.803243	0.315302	0.000685	0.720406
-4.076276	-1.707780	0.320307	0.000883	0.720222
-3.800699	-1.757550	0.325312	0.000831	0.720221
-3.560458	-1.796668	0.330317	0.000786	0.720229
-4.065222	-1.753407	0.335322	0.000880	0.720138
-5.114996	-1.686179	0.340326	0.001075	0.719902
-4.819471	-1.740810	0.345331	0.001020	0.719899
-5.318583	-1.653768	0.350336	0.001112	0.719896
-4.992052	-1.709483	0.355341	0.001051	0.719901
-5.060230	-1.729213	0.360346	0.001064	0.719839
-6.016475	-1.678863	0.365350	0.001242	0.719603
-5.874929	-1.704132	0.370355	0.001215	0.719603
-6.228031	-1.642178	0.375360	0.001280	0.719602
-5.984320	-1.681999	0.380365	0.001235	0.719610
-6.062635	-1.674052	0.385370	0.001249	0.719598
-5.955991	-1.791337	0.390374	0.001229	0.719405
-6.675229	-1.731785	0.395379	0.001363	0.719270
-7.014275	-1.672888	0.400384	0.001426	0.719268
-6.860118	-1.697277	0.405389	0.001397	0.719275
-6.896035	-1.694700	0.410394	0.001403	0.719267
-6.892855	-1.692082	0.415398	0.001402	0.719274
-7.257570	-1.749945	0.420403	0.001470	0.719033
-8.312147	-1.598466	0.425408	0.001666	0.718961
-7.506195	-1.740721	0.430413	0.001516	0.718964
-8.002001	-1.656831	0.435418	0.001608	0.718956
-8.251294	-1.608536	0.440422	0.001654	0.718964
-7.809553	-1.690198	0.445427	0.001571	0.718959
-8.136971	-1.652834	0.450432	0.001632	0.718918
-8.439318	-1.735579	0.455437	0.001688	0.718649
-8.505986	-1.729303	0.460442	0.001700	0.718639
-8.924808	-1.649866	0.465446	0.001778	0.718649
-9.065620	-1.625203	0.470451	0.001804	0.718648
-9.013618	-1.638599	0.475456	0.001794	0.718641
-8.790743	-1.675033	0.480461	0.001752	0.718648
-9.193884	-1.649674	0.485466	0.001827	0.718557
-9.727357	-1.654660	0.490470	0.001926	0.718360
-9.210402	-1.749087	0.495475	0.001829	0.718355
-10.119656	-1.590443	0.500480	0.001998	0.718349
-9.941028	-1.617260	0.505485	0.001965	0.718360
-9.593345	-1.684107	0.510490	0.001900	0.718351
-9.697518	-1.662175	0.515494	0.001919	0.718358
-9.871124	-1.689811	0.520499	0.001951	0.718243
-10.690321	-1.660373	0.525504	0.002103	0.718013
-10.205906	-1.742289	0.530509	0.002013	0.718022
-11.000874	-1.606090	0.535514	0.002161	0.718012
-10.985453	-1.604157	0.540518	0.002157	0.718022
-10.641306	-1.667727	0.545523	0.002093	0.718018
-10.898622	-1.625986	0.550528	0.002141	0.718010
-10.645208	-1.684260	0.555533	0.002093	0.717985
-11.512042	-1.675158	0.560538	0.002254	0.717698
-11.570952	-1.660106	0.565542	0.002265	0.717708
-12.014422	-1.583271	0.570547	0.002347	0.717704
-11.816638	-1.619824	0.575552	0.002310	0.717702
-11.711131	-1.633939	0.580557	0.002290	0.717712
-11.851994	-1.614162	0.585562	0.002316	0.717702
-11.657393	-1.648687	0.590566	0.002280	0.717703
-11.618702	-1.741282	0.595571	0.002272	0.717534
-13.080279	-1.559367	0.600576	0.002544	0.717379
-12.799855	-1.605430	0.605581	0.002492	0.717387
-12.736153	-1.621732	0.610586	0.002480	0.717378
-12.555180	-1.653199	0.615590	0.002446	0.717380
-12.750713	-1.619142	0.620595	0.002482	0.717379
-12.904917	-1.591736	0.625600	0.002510	0.717379
-12.515364	-1.658461	0.630605	0.002437	0.717385
-12.963267	-1.717534	0.635610	0.002521	0.717111
-13.535568	-1.628201	0.640614	0.002627	0.717087
-13.456420	-1.644136	0.645619	0.002612	0.717083
-13.244183	-1.682751	0.650624	0.002572	0.717082
-13.625801	-1.610971	0.655629	0.002643	0.717090
-13.619001	-1.617057	0.660634	0.002641	0.717081
-13.446093	-1.645786	0.665638	0.002609	0.717086
-13.949459	-1.699097	0.670643	0.002702	0.716804
-14.682060	-1.594177	0.675648	0.002838	0.716753
-14.189661	-1.677926	0.680653	0.002746	0.716762
-14.535134	-1.620393	0.685658	0.002810	0.716754
-14.859644	-1.559377	0.690662	0.002871	0.716761
-14.356971	-1.651699	0.695667	0.002777	0.716756
-14.460293	-1.636234	0.700672	0.002796	0.716751
-14.800237	-1.626806	0.705677	0.002859	0.716650
-15.628682	-1.586130	0.710682	0.003013	0.716439
-14.975063	-1.697734	0.715686	0.002891	0.716449
-15.299757	-1.640312	0.720691	0.002951	0.716449
-15.673253	-1.575931	0.725696	0.003020	0.716445
-14.932000	-1.705353	0.730701	0.002882	0.716451
-15.103047	-1.679833	0.735706	0.002914	0.716442
-15.411143	-1.675029	0.740710	0.002971	0.716343
-16.409560	-1.602764	0.745715	0.003156	0.716134
-16.011352	-1.677582	0.750720	0.003082	0.716127
-16.265309	-1.627953	0.755725	0.003129	0.716136
-16.351703	-1.616407	0.760730	0.003145	0.716129
-16.156178	-1.650195	0.765734	0.003108	0.716132
-16.080000	-1.664260	0.770739	0.003094	0.716131
-16.166186	-1.670007	0.775744	0.003109	0.716090
-16.432464	-1.725129	0.780749	0.003159	0.715887
-16.959062	-1.635833	0.785754	0.003256	0.715879
-17.312866	-1.569757	0.790758	0.003322	0.715885
-16.719929	-1.677413	0.795763	0.003211	0.715882
-16.916444	-1.641680	0.800768	0.003248	0.715884
-17.078506	-1.611021	0.805773	0.003278	0.715888
-17.171313	-1.661064	0.810778	0.003295	0.715756
-17.751444	-1.662468	0.815782	0.003402	0.715549
-17.670794	-1.677999	0.820787	0.003387	0.715548
-18.375383	-1.554236	0.825792	0.003518	0.715545
-17.777026	-1.657466	0.830797	0.003406	0.715552
-17.374050	-1.735062	0.835802	0.003331	0.715541
-17.975018	-1.625271	0.840806	0.003443	0.715547
-18.182806	-1.687502	0.845811	0.003481	0.715350
-19.151503	-1.577875	0.850816	0.003661	0.715226
-18.668491	-1.659459	0.855821	0.003571	0.715235
-18.944557	-1.614393	0.860826	0.003622	0.715228
-18.840371	-1.630930	0.865830	0.003602	0.715232
-18.600384	-1.674060	0.870835	0.003557	0.715232
-18.939210	-1.616200	0.875840	0.003620	0.715228
-18.741354	-1.711665	0.880845	0.003583	0.715109
-19.725159	-1.639281	0.885850	0.003766	0.714905
-19.543437	-1.670459	0.890854	0.003732	0.714908
-19.686726	-1.644246	0.895859	0.003758	0.714910
-19.601397	-1.663285	0.900864	0.003742	0.714903
-19.517296	-1.673020	0.905869	0.003726	0.714914
-20.100502	-1.573549	0.910874	0.003835	0.714905
-19.829743	-1.667857	0.915878	0.003784	0.714814
-20.513315	-1.648598	0.920883	0.003911	0.714611
-20.819130	-1.596733	0.925888	0.003968	0.714607
-20.820905	-1.593176	0.930893	0.003968	0.714614
-20.298389	-1.689708	0.935898	0.003870	0.714607
-20.589052	-1.635864	0.940902	0.003924	0.714612
-20.754533	-1.607231	0.945907	0.003954	0.714611
-20.602859	-1.640447	0.950912	0.003926	0.714599
-20.861656	-1.753809	0.955917	0.003974	0.714283
-21.530231	-1.639709	0.960922	0.004098	0.714273
-21.689968	-1.609151	0.965926	0.004128	0.714278
-21.235728	-1.689040	0.970931	0.004043	0.714281
-21.708678	-1.607160	0.975936	0.004131	0.714276
-21.491446	-1.642466	0.980941	0.004090	0.714284
-21.570947	-1.635594	0.985946	0.004104	0.714270
-22.173985	-1.678279	0.990950	0.004216	0.713972
-22.383827	-1.642840	0.995955	0.004255	0.713969
-22.469906	-1.629451	1.000960	0.004271	0.713965
-22.072091	-1.694930	1.005965	0.004197	0.713976
-22.667832	-1.593762	1.010970	0.004307	0.713967
-22.591154	-1.605758	1.015974	0.004293	0.713971
-22.244412	-1.666811	1.020979	0.004228	0.713973
-23.056649	-1.652802	1.025984	0.004379	0.713714
-23.563559	-1.593484	1.030989	0.004473	0.713652
-23.174864	-1.666686	1.035994	0.004400	0.713645
-23.224453	-1.654027	1.040998	0.004409	0.713653
-23.759174	-1.560546	1.046003	0.004509	0.713650
-23.701095	-1.573900	1.051008	0.004497	0.713645
-23.036115	-1.689378	1.056013	0.004373	0.713651
-23.678370	-1.600723	1.061018	0.004493	0.713601
-24.312115	-1.609807	1.066022	0.004610	0.713358
-23.823586	-1.695891	1.071027	0.004519	0.713361
-24.503113	-1.578531	1.076032	0.004645	0.713354
-24.142189	-1.637563	1.081037	0.004578	0.713365
-23.996269	-1.667901	1.086042	0.004551	0.713357
-24.440014	-1.587292	1.091046	0.004633	0.713360
-24.353864	-1.609963	1.096051	0.004617	0.713346
-24.909163	-1.674866	1.101056	0.004720	0.713021
-24.994850	-1.656641	1.106061	0.004735	0.713027
-25.804841	-1.516148	1.111066	0.004886	0.713020
-25.160504	-1.628349	1.116070	0.004766	0.713026
-24.757794	-1.699968	1.121075	0.004690	0.713027
-25.306690	-1.607094	1.126080	0.004792	0.713017
-25.236364	-1.615490	1.131085	0.004779	0.713026
-25.585070	-1.661689	1.136090	0.004844	0.712811
-26.446069	-1.561344	1.141094	0.005004	0.712706
-26.196586	-1.603664	1.146099	0.004957	0.712711
-26.293257	-1.587835	1.151104	0.004975	0.712708
-26.060218	-1.626088	1.156109	0.004931	0.712715
-26.188259	-1.607374	1.161114	0.004955	0.712708
-26.331993	-1.580376	1.166118	0.004981	0.712711
-26.194400	-1.616597	1.171123	0.004955	0.712688
-26.938603	-1.636511	1.176128	0.005094	0.712385
-27.173213	-1.591518	1.181133	0.005137	0.712392
-27.247343	-1.582643	1.186138	0.005150	0.712384
-27.048704	-1.618178	1.191142	0.005113	0.712384
-27.256046	-1.581256	1.196147	0.005152	0.712384
-27.294201	-1.576676	1.201152	0.005158	0.712381
-27.008799	-1.622929	1.206157	0.005105	0.712390
-27.415688	-1.614705	1.211162	0.005180	0.712263
-28.522573	-1.501714	1.216166	0.005386	0.712095
-27.409194	-1.700910	1.221171	0.005179	0.712094
-27.852289	-1.623743	1.226176	0.005261	0.712091
-28.418392	-1.520858	1.231181	0.005366	0.712096
-27.903528	-1.616892	1.236186	0.005270	0.712088
-27.748127	-1.642844	1.241190	0.005241	0.712092
-27.846138	-1.682267	1.246195	0.005259	0.711979
-29.167965	-1.558066	1.251200	0.005505	0.711757
-28.619383	-1.652319	1.256205	0.005402	0.711765
-29.187890	-1.554993	1.261210	0.005508	0.711758
-29.302929	-1.531073	1.266214	0.005529	0.711765
-28.852888	-1.612425	1.271219	0.005445	0.711763
-29.264386	-1.543078	1.276224	0.005521	0.711756
-28.731145	-1.633109	1.281229	0.005422	0.711766
-28.938865	-1.716514	1.286234	0.005460	0.711526
-30.045651	-1.555237	1.291238	0.005666	0.711455
-29.972692	-1.568380	1.296243	0.005652	0.711456
-29.935037	-1.577461	1.301248	0.005645	0.711451
-29.615501	-1.630316	1.306253	0.005585	0.711460
-29.742829	-1.614381	1.311258	0.005608	0.711447
-29.960753	-1.572363	1.316262	0.005649	0.711454
-29.770812	-1.704237	1.321267	0.005613	0.711259
-30.794422	-1.584087	1.326272	0.005803	0.711135
-30.799430	-1.578447	1.331277	0.005804	0.711145
-30.929081	-1.560099	1.336282	0.005828	0.711136
-30.657673	-1.607080	1.341286	0.005777	0.711139
-30.476174	-1.639838	1.346291	0.005743	0.711139
-31.182722	-1.517006	1.351296	0.005874	0.711134
-30.988976	-1.595473	1.356301	0.005838	0.711046
-31.482985	-1.597395	1.361306	0.005930	0.710867
-31.651399	-1.568267	1.366310	0.005961	0.710866
-31.625271	-1.572634	1.371315	0.005956	0.710867
-31.636170	-1.574430	1.376320	0.005957	0.710860
-31.297969	-1.630539	1.381325	0.005894	0.710869
-31.488182	-1.599912	1.386330	0.005929	0.710863
-31.606535	-1.646980	1.391334	0.005951	0.710727
-32.394965	-1.606550	1.396339	0.006098	0.710528
-32.385569	-1.609772	1.401344	0.006096	0.710525
-32.058959	-1.663898	1.406349	0.006035	0.710534
-32.258938	-1.632700	1.411354	0.006071	0.710526
-32.777884	-1.537627	1.416358	0.006168	0.710532
-32.658258	-1.559438	1.421363	0.006145	0.710531
-32.556252	-1.640819	1.426368	0.006126	0.710405
-33.617384	-1.545335	1.431373	0.006323	0.710219
-33.505320	-1.568845	1.436378	0.006302	0.710212
-33.668764	-1.537477	1.441382	0.006332	0.710217
-33.311596	-1.603027	1.446387	0.006266	0.710214
-33.824951	-1.513636	1.451392	0.006361	0.710210
-33.727822	-1.525580	1.456397	0.006343	0.710221
-33.541119	-1.564110	1.461402	0.006307	0.710211
-33.628399	-1.655931	1.466406	0.006324	0.709997
-34.636976	-1.528685	1.471411	0.006511	0.709893
-34.498558	-1.556618	1.476416	0.006485	0.709887
-34.161774	-1.612133	1.481421	0.006422	0.709896
-34.799245	-1.501753	1.486426	0.006540	0.709891
-34.285872	-1.591784	1.491430	0.006445	0.709894
-34.100878	-1.625011	1.496435	0.006410	0.709894
-34.633423	-1.575995	1.501440	0.006509	0.709803
-35.172785	-1.582539	1.506445	0.006609	0.709598
-35.028124	-1.612598	1.511450	0.006582	0.709590
-35.662369	-1.497833	1.516454	0.006699	0.709594
-35.468078	-1.530844	1.521459	0.006663	0.709598
-35.308718	-1.563289	1.526464	0.006633	0.709590
-35.230880	-1.572815	1.531469	0.006618	0.709599
-35.672873	-1.497698	1.536474	0.006700	0.709592
-35.731567	-1.625135	1.541478	0.006711	0.709317
-36.049167	-1.593207	1.546483	0.006770	0.709268
-36.677887	-1.483871	1.551488	0.006887	0.709263
-36.188311	-1.566624	1.556493	0.006795	0.709273
-36.066010	-1.592307	1.561498	0.006772	0.709266
-36.031331	-1.598668	1.566502	0.006766	0.709266
-36.216532	-1.564476	1.571507	0.006800	0.709269
-36.606955	-1.601457	1.576512	0.006872	0.709056
-37.356464	-1.516206	1.581517	0.007011	0.708960
-37.100911	-1.565363	1.586522	0.006964	0.708953
-37.080975	-1.567928	1.591526	0.006960	0.708955
-37.044573	-1.571711	1.596531	0.006953	0.708961
-37.173579	-1.554163	1.601536	0.006976	0.708951
-37.010879	-1.579325	1.606541	0.006946	0.708959
-37.155673	-1.619734	1.611546	0.006972	0.708827
-38.414001	-1.489995	1.616550	0.007206	0.708638
-38.124143	-1.540629	1.621555	0.007152	0.708641
-37.988719	-1.568336	1.626560	0.007127	0.708634
-37.853387	-1.588351	1.631565	0.007101	0.708643
-37.843454	-1.594237	1.636570	0.007099	0.708635
-38.165481	-1.536283	1.641574	0.007159	0.708637
-37.660247	-1.660605	1.646579	0.007065	0.708569
-38.730032	-1.585192	1.651584	0.007263	0.708338
-38.749563	-1.575036	1.656589	0.007267	0.708352
-38.876377	-1.556899	1.661594	0.007290	0.708344
-38.571893	-1.609674	1.666598	0.007233	0.708347
-38.781333	-1.572058	1.671603	0.007272	0.708348
-38.905497	-1.553536	1.676608	0.007295	0.708342
-39.003529	-1.618729	1.681613	0.007313	0.708177
-40.249890	-1.481679	1.686618	0.007544	0.708007
-39.836009	-1.554811	1.691622	0.007467	0.708008
-39.550142	-1.604582	1.696627	0.007414	0.708011
-39.858538	-1.552598	1.701632	0.007471	0.708006
-39.718301	-1.574543	1.706637	0.007444	0.708012
-39.600101	-1.599567	1.711642	0.007422	0.708005
-39.803315	-1.595021	1.716646	0.007460	0.707942
-40.668281	-1.563859	1.721651	0.007621	0.707696
-40.469196	-1.601548	1.726656	0.007583	0.707692
-40.374121	-1.614045	1.731661	0.007565	0.707701
-40.793093	-1.543594	1.736666	0.007643	0.707693
-41.109802	-1.488375	1.741670	0.007702	0.707691
-40.794389	-1.542168	1.746675	0.007643	0.707697
-40.741541	-1.554376	1.751680	0.007633	0.707692
-41.123567	-1.624883	1.756685	0.007703	0.707414
-41.788293	-1.528944	1.761690	0.007827	0.707369
-41.732847	-1.537686	1.766694	0.007816	0.707372
-41.625874	-1.555145	1.771699	0.007796	0.707376
-42.087257	-1.478142	1.776704	0.007882	0.707366
-41.582535	-1.563037	1.781709	0.007788	0.707377
-41.311836	-1.615047	1.786714	0.007737	0.707370
-41.839879	-1.591846	1.791718	0.007835	0.707228
-42.580389	-1.532661	1.796723	0.007972	0.707082
-42.339171	-1.577744	1.801728	0.007927	0.707079
-42.267211	-1.587214	1.806733	0.007914	0.707086
-42.313068	-1.583536	1.811738	0.007922	0.707077
-42.246442	-1.593960	1.816742	0.007909	0.707081
-42.610948	-1.527030	1.821747	0.007977	0.707085
-42.803559	-1.597984	1.826752	0.008012	0.706874
-43.383215	-1.554686	1.831757	0.008120	0.706754
-43.520805	-1.533411	1.836762	0.008145	0.706748
-43.757382	-1.492354	1.841766	0.008189	0.706747
-43.432373	-1.550197	1.846771	0.008128	0.706747
-43.362290	-1.565163	1.851776	0.008115	0.706743
-43.414284	-1.551996	1.856781	0.008125	0.706751
-43.667276	-1.521885	1.861786	0.008171	0.706722
-43.986176	-1.604139	1.866790	0.008231	0.706443
-43.968702	-1.605921	1.871795	0.008227	0.706446
-44.510765	-1.513592	1.876800	0.008328	0.706438
-44.197079	-1.565301	1.881805	0.008269	0.706447
-44.067875	-1.592592	1.886810	0.008245	0.706439
-44.548339	-1.506777	1.891814	0.008334	0.706439
-44.321029	-1.560217	1.896819	0.008291	0.706414
-44.896597	-1.603137	1.901824	0.008398	0.706122
-45.157176	-1.551587	1.906829	0.008446	0.706133
-45.162207	-1.554288	1.911834	0.008447	0.706126
-45.035678	-1.576054	1.916838	0.008423	0.706128
-45.175717	-1.551271	1.921843	0.008449	0.706128
-45.416454	-1.512731	1.926848	0.008494	0.706120
-45.013492	-1.587501	1.931853	0.008418	0.706115
-45.376375	-1.652204	1.936858	0.008486	0.705855
-46.036538	-1.532140	1.941862	0.008608	0.705860
-45.759517	-1.580967	1.946867	0.008556	0.705862
-45.527497	-1.626157	1.951872	0.008513	0.705855
-45.993772	-1.538212	1.956877	0.008599	0.705865
-46.217797	-1.500980	1.961882	0.008641	0.705860
-46.007332	-1.611821	1.966886	0.008601	0.705713
-46.823044	-1.558332	1.971891	0.008753	0.705529
-46.672286	-1.589034	1.976896	0.008725	0.705522
-46.695540	-1.580803	1.981901	0.008729	0.705530
-46.685280	-1.587700	1.986906	0.008727	0.705521
-46.985885	-1.532005	1.991910	0.008782	0.705525
-46.809464	-1.563326	1.996915	0.008749	0.705526
-47.517830	-1.559266	2.001920	0.008881	0.705281

-47.659347	-1.568832	2.011917	0.008907	0.705212
-47.857787	-1.535215	2.021914	0.008943	0.705209
-47.681735	-1.566108	2.031910	0.008910	0.705211
-47.651306	-1.571738	2.041907	0.008903	0.705212
-47.478990	-1.604255	2.051904	0.008871	0.705209
-47.702516	-1.564613	2.061901	0.008912	0.705210
-47.761527	-1.554416	2.071898	0.008922	0.705210
-47.841116	-1.538958	2.081894	0.008937	0.705214
-47.806244	-1.547438	2.091891	0.008930	0.705210
-47.828566	-1.543898	2.101888	0.008933	0.705211
-47.680090	-1.571195	2.111885	0.008905	0.705210
-47.093448	-1.521177	2.121882	0.008795	0.705522
-46.793130	-1.573250	2.131878	0.008739	0.705526
-46.949389	-1.544513	2.141875	0.008767	0.705529
-46.927960	-1.549549	2.151872	0.008763	0.705527
-47.222205	-1.500019	2.161869	0.008817	0.705523
-46.357058	-1.556415	2.171866	0.008655	0.705721
-46.092064	-1.532606	2.181862	0.008606	0.705864
-45.927209	-1.563715	2.191859	0.008574	0.705862
-45.997993	-1.551419	2.201856	0.008587	0.705862
-46.032460	-1.533124	2.211853	0.008593	0.705888
-45.328620	-1.540573	2.221850	0.008461	0.706126
-45.089265	-1.582164	2.231846	0.008416	0.706129
-45.294819	-1.546388	2.241843	0.008454	0.706129
-45.185443	-1.531805	2.251840	0.008433	0.706198
-44.431555	-1.544968	2.261837	0.008292	0.706443
-44.362694	-1.557838	2.271834	0.008279	0.706443
-44.759745	-1.486916	2.281830	0.008352	0.706444
-43.676554	-1.570676	2.291827	0.008150	0.706665
-43.426500	-1.574021	2.301824	0.008103	0.706749
-43.706019	-1.525763	2.311821	0.008154	0.706747
-43.456672	-1.566797	2.321818	0.008107	0.706755
-42.757317	-1.528485	2.331814	0.007977	0.707083
-42.466711	-1.580724	2.341811	0.007922	0.707083
-42.563750	-1.565423	2.351808	0.007939	0.707080
-42.518368	-1.529922	2.361805	0.007930	0.707169
-41.532623	-1.604129	2.371802	0.007746	0.707373
-41.846873	-1.548087	2.381798	0.007804	0.707374
-41.908250	-1.538637	2.391795	0.007815	0.707372
-41.326827	-1.500968	2.401792	0.007706	0.707657
-41.046177	-1.533197	2.411789	0.007654	0.707694
-40.831806	-1.571144	2.421786	0.007613	0.707695
-40.781572	-1.498707	2.431782	0.007603	0.707860
-39.828151	-1.593431	2.441779	0.007425	0.708011
-40.168023	-1.533954	2.451776	0.007488	0.708010
-40.172756	-1.530587	2.461773	0.007488	0.708016
-39.462677	-1.491881	2.471770	0.007355	0.708349
-39.167012	-1.545719	2.481766	0.007300	0.708347
-39.007785	-1.573757	2.491763	0.007270	0.708349
-38.827447	-1.527004	2.501760	0.007236	0.708508
-38.154675	-1.583176	2.511757	0.007110	0.708637
-38.275790	-1.560897	2.521754	0.007132	0.708639
-38.451034	-1.528229	2.531750	0.007164	0.708643
-37.600611	-1.522418	2.541747	0.007005	0.708959
-37.422519	-1.555143	2.551744	0.006971	0.708959
-37.378124	-1.565680	2.561741	0.006963	0.708954
-37.186299	-1.519067	2.571738	0.006926	0.709117
-36.553827	-1.557918	2.581734	0.006808	0.709266
-36.609476	-1.549259	2.591731	0.006818	0.709264
-36.584527	-1.540553	2.601728	0.006813	0.709292
-35.597356	-1.564659	2.611725	0.006628	0.709597
-35.604824	-1.563415	2.621722	0.006629	0.709597
-35.908760	-1.508671	2.631718	0.006685	0.709600
-35.201372	-1.547060	2.641715	0.006553	0.709776
-34.901856	-1.540608	2.651712	0.006497	0.709897
-34.783110	-1.563303	2.661709	0.006474	0.709895
-34.913220	-1.524722	2.671706	0.006498	0.709926
-33.867458	-1.565572	2.681702	0.006302	0.710218
-33.867082	-1.565296	2.691699	0.006302	0.710220
-33.966456	-1.549902	2.701696	0.006320	0.710216
-33.665755	-1.520424	2.711693	0.006263	0.710383
-33.040177	-1.559814	2.721690	0.006146	0.710529
-33.186075	-1.532688	2.731686	0.006173	0.710532
-32.910883	-1.570234	2.741683	0.006121	0.710556
-32.428001	-1.500611	2.751680	0.006031	0.710868
-32.102364	-1.560879	2.761677	0.005969	0.710864
-32.324832	-1.521595	2.771674	0.006010	0.710865
-31.695870	-1.554447	2.781670	0.005893	0.711024
-31.330780	-1.563205	2.791667	0.005824	0.711137
-31.351431	-1.560551	2.801664	0.005827	0.711136
-31.341992	-1.542268	2.811661	0.005825	0.711177
-30.808639	-1.499202	2.821658	0.005725	0.711454
-30.329907	-1.584517	2.831654	0.005636	0.711455
-30.579334	-1.539999	2.841651	0.005681	0.711456
-29.958411	-1.525530	2.851648	0.005565	0.711706
-29.552986	-1.571794	2.861645	0.005489	0.711759
-29.808328	-1.526341	2.871642	0.005536	0.711760
-29.348053	-1.547056	2.881638	0.005450	0.711883
-28.788633	-1.544134	2.891635	0.005345	0.712089
-28.559195	-1.584632	2.901632	0.005302	0.712091
-28.924630	-1.520189	2.911629	0.005370	0.712090
-28.108480	-1.538580	2.921626	0.005217	0.712345
-27.841109	-1.565160	2.931622	0.005167	0.712387
-27.889211	-1.556360	2.941619	0.005175	0.712389
-27.926000	-1.491586	2.951616	0.005181	0.712506
-26.945178	-1.566870	2.961613	0.004998	0.712705
-27.124513	-1.535903	2.971610	0.005031	0.712704
-27.078372	-1.536712	2.981606	0.005022	0.712720
-26.409747	-1.505604	2.991603	0.004897	0.713020
-26.112981	-1.559821	3.001600	0.004841	0.713018
-26.249166	-1.535641	3.011597	0.004866	0.713019
-25.971925	-1.476331	3.021594	0.004814	0.713237
-25.224620	-1.549772	3.031590	0.004674	0.713356
-25.505107	-1.498900	3.041587	0.004726	0.713359
-24.938232	-1.579868	3.051584	0.004620	0.713400
-24.463266	-1.539097	3.061581	0.004531	0.713650
-24.437073	-1.544752	3.071578	0.004525	0.713650
-24.379381	-1.554604	3.081574	0.004514	0.713651
-24.008526	-1.530544	3.091571	0.004444	0.713832
-23.510584	-1.551242	3.101568	0.004351	0.713968
-23.615123	-1.532032	3.111565	0.004370	0.713970
-23.410525	-1.557439	3.121562	0.004332	0.713993
-22.567750	-1.564656	3.131558	0.004174	0.714278
-22.514594	-1.572321	3.141555	0.004164	0.714283
-22.546099	-1.569310	3.151552	0.004169	0.714278
-22.622835	-1.472387	3.161549	0.004183	0.714445
-21.732193	-1.547434	3.171546	0.004016	0.714612
-21.625568	-1.565096	3.181542	0.003996	0.714616
-21.635994	-1.564424	3.191539	0.003997	0.714614
-20.937506	-1.553241	3.201536	0.003867	0.714885
-20.993564	-1.530422	3.211533	0.003877	0.714911
-20.971487	-1.534163	3.221530	0.003872	0.714912
-20.795781	-1.484105	3.231526	0.003839	0.715075
-19.996015	-1.546226	3.241523	0.003689	0.715235
-19.942554	-1.555793	3.251520	0.003679	0.715236
-20.193927	-1.496991	3.261517	0.003725	0.715265
-19.080835	-1.554408	3.271514	0.003517	0.715546
-18.920434	-1.581449	3.281510	0.003487	0.715550
-19.190871	-1.534223	3.291507	0.003537	0.715549
-18.770588	-1.520008	3.301504	0.003458	0.715726
-17.890546	-1.595833	3.311501	0.003293	0.715888
-18.179730	-1.545031	3.321498	0.003347	0.715887
-18.064771	-1.567880	3.331494	0.003325	0.715884
-17.690469	-1.549727	3.341491	0.003255	0.716053
-17.309003	-1.576107	3.351488	0.003183	0.716136
-17.609431	-1.524171	3.361485	0.003238	0.716134
-17.072813	-1.575856	3.371482	0.003138	0.716222
-16.416000	-1.578187	3.381478	0.003015	0.716450
-16.407588	-1.578860	3.391475	0.003013	0.716453
-16.546641	-1.556067	3.401472	0.003038	0.716450
-15.883984	-1.548305	3.411469	0.002914	0.716700
-15.662048	-1.560637	3.421466	0.002873	0.716755
-15.537581	-1.582692	3.431462	0.002849	0.716756
-15.216492	-1.590925	3.441459	0.002789	0.716854
-14.292238	-1.637266	3.451456	0.002616	0.717089
-14.480559	-1.606213	3.461453	0.002650	0.717085
-14.261704	-1.645752	3.471450	0.002609	0.717085
-14.685752	-1.513688	3.481446	0.002688	0.717198
-13.269168	-1.672361	3.491443	0.002423	0.717384
-13.640265	-1.606857	3.501440	0.002492	0.717384
-13.610310	-1.614289	3.511437	0.002486	0.717381
-13.068979	-1.596162	3.521434	0.002384	0.717609
-12.592048	-1.631969	3.531430	0.002295	0.717707
-12.588712	-1.633198	3.541427	0.002294	0.717706
-12.655528	-1.620548	3.551424	0.002306	0.717709
-12.049760	-1.575036	3.561421	0.002192	0.718013
-11.676936	-1.639741	3.571418	0.002123	0.718017
-11.962440	-1.588654	3.581414	0.002175	0.718019
-11.372152	-1.615459	3.591411	0.002065	0.718175
-10.911881	-1.606107	3.601408	0.001978	0.718356
-10.691115	-1.646299	3.611405	0.001937	0.718355
-10.783376	-1.631333	3.621402	0.001953	0.718354
-10.290640	-1.637634	3.631398	0.001861	0.718515
-10.029015	-1.618473	3.641395	0.001812	0.718646
-10.055637	-1.614762	3.651392	0.001816	0.718645
-9.976728	-1.614563	3.661389	0.001801	0.718674
-9.235929	-1.600244	3.671386	0.001663	0.718964
-9.137876	-1.618580	3.681382	0.001644	0.718963
-8.678797	-1.700026	3.691379	0.001558	0.718965
-9.009429	-1.564008	3.701376	0.001619	0.719118
-7.962879	-1.673126	3.711373	0.001423	0.719271
-8.180835	-1.635815	3.721370	0.001463	0.719270
-8.064637	-1.656313	3.731366	0.001441	0.719271
-7.430863	-1.623512	3.741363	0.001323	0.719559
-7.376371	-1.613314	3.751360	0.001312	0.719599
-7.010680	-1.679869	3.761357	0.001243	0.719598
-7.142038	-1.628641	3.771354	0.001267	0.719653
-6.219411	-1.669134	3.781350	0.001095	0.719898
-6.319739	-1.651942	3.791347	0.001113	0.719898
-6.396394	-1.637815	3.801344	0.001127	0.719900
-5.771277	-1.654641	3.811341	0.001010	0.720087
-5.612296	-1.616487	3.821338	0.000980	0.720219
-5.294679	-1.671065	3.831334	0.000920	0.720224
-5.181111	-1.690933	3.841331	0.000898	0.720226
-4.792821	-1.628736	3.851328	0.000826	0.720485
-4.408381	-1.668770	3.861325	0.000753	0.720542
-4.620214	-1.632794	3.871322	0.000792	0.720540
-4.227224	-1.666128	3.881318	0.000719	0.720613
-3.364933	-1.682225	3.891315	0.000558	0.720885
-3.344002	-1.688097	3.901312	0.000553	0.720881
-3.396638	-1.681266	3.911309	0.000562	0.720877
-3.403300	-1.642857	3.921306	0.000563	0.720952
-2.628625	-1.693910	3.931302	0.000418	0.721124
-2.766577	-1.667913	3.941299	0.000443	0.721127
-2.538547	-1.710307	3.951296	0.000400	0.721125
-2.129207	-1.647665	3.961293	0.000324	0.721392
-1.930162	-1.660408	3.971290	0.000286	0.721438
-1.691364	-1.704123	3.981286	0.000241	0.721437
-1.735727	-1.635271	3.991283	0.000249	0.721558
-1.364039	-1.606807	4.001280	0.000179	0.721745
-1.319071	-1.615092	4.011277	0.000170	0.721745
-1.218818	-1.573794	4.021274	0.000151	0.721862
-0.809018	-1.540853	4.031270	0.000074	0.722071
-0.760950	-1.548655	4.041267	0.000065	0.722074
-0.717060	-1.475323	4.051264	0.000056	0.722234
-0.601187	-1.429918	4.061261	0.000034	0.722365
-0.507300	-1.435885	4.071258	0.000016	0.722387
-0.513257	-1.281603	4.081254	0.000016	0.722689
-0.492668	-1.284869	4.091251	0.000012	0.722691
-0.305923	-1.163519	4.101248	-0.000024	0.722995
-0.256070	-1.166416	4.111245	-0.000034	0.723008
-0.393434	-0.975092	4.121242	-0.000009	0.723336
-0.147980	-0.979087	4.131238	-0.000055	0.723415
-0.140616	-0.870666	4.141235	-0.000057	0.723631
-0.086581	-0.781412	4.151232	-0.000067	0.723826
-0.155948	-0.690948	4.161229	-0.000055	0.723980
-0.103886	-0.559627	4.171226	-0.000065	0.724256
0.018117	-0.469171	4.181222	-0.000089	0.724477
-0.002110	-0.363185	4.191219	-0.000086	0.724678
0.153146	-0.285254	4.201216	-0.000115	0.724885
0.254198	-0.139457	4.211213	-0.000135	0.725207
0.244940	-0.017808	4.221210	-0.000133	0.725442
0.267099	0.110245	4.231206	-0.000138	0.725701
0.000000	0.307304	4.241203	-0.000089	0.725995

0.208434	0.876120	4.246208	-0.000129	0.727178
0.417865	2.114463	4.251213	-0.000169	0.729661
0.537431	3.956424	4.256218	-0.000192	0.733274
0.585493	6.356018	4.261222	-0.000203	0.737917
1.048212	9.202786	4.266227	-0.000291	0.743525
1.319437	12.567331	4.271232	-0.000344	0.750006
1.941435	16.318167	4.276237	-0.000463	0.757272
2.096056	20.562714	4.281242	-0.000495	0.765230
2.309336	25.201703	4.286246	-0.000538	0.773849
2.702642	30.166072	4.291251	-0.000615	0.783019
3.275971	35.451997	4.296256	-0.000725	0.792716
3.708643	41.081778	4.301261	-0.000810	0.802859
3.645845	47.100877	4.306266	-0.000802	0.813401
4.172291	53.285231	4.311270	-0.000904	0.824272
4.679675	59.767237	4.316275	-0.001003	0.835500
4.998473	66.471912	4.321280	-0.001067	0.846897
5.595447	73.370629	4.326285	-0.001183	0.858543
6.339368	80.458211	4.331290	-0.001327	0.870384
6.930720	87.737435	4.336294	-0.001442	0.882329
7.749993	95.172306	4.341299	-0.001599	0.894425
8.303438	102.798216	4.346304	-0.001708	0.906585
8.749097	110.598114	4.351309	-0.001796	0.918823
9.240198	118.491875	4.356314	-0.001893	0.931055
9.834156	126.480855	4.361318	-0.002009	0.943299
10.511563	134.585217	4.366323	-0.002141	0.955577
11.207612	142.750914	4.371328	-0.002276	0.967794
12.232627	150.960845	4.376333	-0.002472	0.980006
13.427847	159.247794	4.381338	-0.002701	0.992219
13.915983	167.675625	4.386342	-0.002797	1.004308
15.075138	176.052368	4.391347	-0.003019	1.016344
15.884863	184.524486	4.396352	-0.003175	1.028286
16.548807	193.071860	4.401357	-0.003305	1.040159
17.177551	201.653357	4.406362	-0.003428	1.051936
17.702739	210.265012	4.411366	-0.003531	1.063598
18.472090	218.886760	4.416371	-0.003681	1.075202
18.676702	227.566780	4.421376	-0.003725	1.086631
19.737444	236.132328	4.426381	-0.003928	1.097983
20.509120	244.755794	4.431386	-0.004078	1.109229
20.937462	253.424726	4.436390	-0.004163	1.120344
21.544061	262.074048	4.441395	-0.004282	1.131364
22.121226	270.716671	4.446400	-0.004395	1.142263
22.863909	279.360284	4.451405	-0.004540	1.153094
23.601673	287.967664	4.456410	-0.004683	1.163779
24.156385	296.589975	4.461414	-0.004792	1.174347
25.114477	305.141811	4.466419	-0.004976	1.184818
25.834731	313.736839	4.471424	-0.005116	1.195200
26.571102	322.293889	4.476429	-0.005259	1.205451
27.266438	330.879424	4.481434	-0.005395	1.215640
27.749085	339.463634	4.486438	-0.005490	1.225701
28.385004	348.048788	4.491443	-0.005615	1.235710
29.188588	356.538976	4.496448	-0.005770	1.245563
29.869435	365.071688	4.501453	-0.005903	1.255363
30.290023	373.629254	4.506458	-0.005987	1.265065
30.477614	382.203079	4.511462	-0.006028	1.274668
31.167349	390.673928	4.516467	-0.006162	1.284178
31.868856	399.141226	4.521472	-0.006298	1.293617
32.302452	407.627294	4.526477	-0.006385	1.302958
32.972692	416.165633	4.531482	-0.006515	1.312332
33.185820	424.677650	4.536486	-0.006561	1.321528
33.681567	433.088447	4.541491	-0.006659	1.330604
34.287715	441.473672	4.546496	-0.006778	1.339610
34.793647	449.866508	4.551501	-0.006877	1.348547
35.302581	458.269738	4.556506	-0.006978	1.357435
35.641116	466.652273	4.561510	-0.007047	1.366215
36.160247	475.047343	4.566515	-0.007149	1.374982
36.394584	483.434461	4.571520	-0.007199	1.383637
37.170323	491.760135	4.576525	-0.007349	1.392267
37.625856	500.120181	4.581530	-0.007439	1.400825
38.227780	508.430227	4.586534	-0.007557	1.409305
38.647652	516.796403	4.591539	-0.007641	1.417759
39.139409	525.107209	4.596544	-0.007738	1.426120
39.805902	533.419459	4.601549	-0.007868	1.434462
40.128740	541.756986	4.606554	-0.007934	1.442725
40.652739	550.047863	4.611558	-0.008037	1.450927
41.270822	558.348320	4.616563	-0.008158	1.459107
41.620363	566.660659	4.621568	-0.008228	1.467211
41.978561	575.027843	4.626573	-0.008301	1.475323
42.389040	583.302636	4.631578	-0.008383	1.483311
42.833695	591.573513	4.636582	-0.008471	1.491258
43.220970	599.853436	4.641587	-0.008549	1.499162
43.819389	608.094681	4.646592	-0.008666	1.507021
44.461208	616.343657	4.651597	-0.008791	1.514852
45.165399	624.568996	4.656602	-0.008928	1.522631
45.451751	632.847258	4.661606	-0.008987	1.530355
45.779831	641.133879	4.666611	-0.009054	1.538055
46.135060	649.382629	4.671616	-0.009126	1.545685
46.546310	657.664424	4.676621	-0.009208	1.553317
46.748218	665.922290	4.681626	-0.009251	1.560858
47.021215	674.159307	4.686630	-0.009308	1.568354
47.469108	682.389315	4.691635	-0.009397	1.575834
47.887846	690.591122	4.696640	-0.009480	1.583249
47.990130	698.866393	4.701645	-0.009505	1.590649
48.775669	707.031956	4.706650	-0.009657	1.598016
49.225671	715.213421	4.711654	-0.009746	1.605314
50.027357	723.400105	4.716659	-0.009901	1.612633
50.261720	731.640475	4.721664	-0.009950	1.619887
50.618327	739.861599	4.726669	-0.010022	1.627108
51.153513	748.118550	4.731674	-0.010128	1.634353
51.583672	756.285161	4.736678	-0.010213	1.641474
51.930269	764.488173	4.741683	-0.010284	1.648583
52.408171	772.674552	4.746688	-0.010378	1.655666
52.821240	780.854809	4.751693	-0.010461	1.662704
53.378824	789.022428	4.756698	-0.010570	1.669721
53.683751	797.231295	4.761702	-0.010633	1.676709
54.249700	805.393166	4.766707	-0.010743	1.683664
54.432768	813.608811	4.771712	-0.010783	1.690584
54.902863	821.776334	4.776717	-0.010876	1.697473
55.490750	829.935316	4.781722	-0.010991	1.704343
55.756440	838.149598	4.786726	-0.011046	1.711189
56.170848	846.345846	4.791731	-0.011129	1.718012
56.421646	854.512636	4.796736	-0.011182	1.724762
57.024715	862.654697	4.801741	-0.011299	1.731511
57.374011	870.849997	4.806746	-0.011370	1.738245
57.142519	879.068579	4.811750	-0.011333	1.744897
57.646004	887.225013	4.816755	-0.011432	1.751567
58.068215	895.373826	4.821760	-0.011516	1.758195
58.303743	903.524795	4.826765	-0.011566	1.764777
58.836506	911.660150	4.831770	-0.011670	1.771358
59.138793	919.820630	4.836774	-0.011732	1.777907
59.680290	927.937955	4.841779	-0.011839	1.784426
59.993938	936.131161	4.846784	-0.011903	1.790954
60.354567	944.306888	4.851789	-0.011975	1.797450
60.743613	952.442141	4.856794	-0.012053	1.803894
60.757259	960.604654	4.861798	-0.012061	1.810290
61.355057	968.722106	4.866803	-0.012178	1.816700
61.608574	976.864229	4.871808	-0.012231	1.823065
61.931070	985.001054	4.876813	-0.012297	1.829411
62.257479	993.157973	4.881818	-0.012363	1.835752
62.556023	1001.270529	4.886822	-0.012424	1.842033
62.729163	1009.441125	4.891827	-0.012462	1.848322
63.254534	1017.557139	4.896832	-0.012565	1.854590
63.592217	1025.683062	4.901837	-0.012634	1.860822
64.006879	1033.812652	4.906842	-0.012717	1.867045
64.195654	1041.990205	4.911846	-0.012757	1.873257
64.500931	1050.119732	4.916851	-0.012820	1.879426
64.741156	1058.236482	4.921856	-0.012870	1.885557
64.936716	1066.378761	4.926861	-0.012912	1.891683
65.181830	1074.522949	4.931866	-0.012963	1.897795
65.510246	1082.616975	4.936870	-0.013030	1.903860
65.692425	1090.774230	4.941875	-0.013070	1.909937
65.864415	1098.908484	4.946880	-0.013107	1.915975
66.414715	1106.962045	4.951885	-0.013215	1.921978
67.053531	1115.051956	4.956890	-0.013340	1.927998
67.247813	1123.205493	4.961894	-0.013381	1.933996
67.394290	1131.347876	4.966899	-0.013414	1.939963
68.045630	1139.416648	4.971904	-0.013541	1.945913
68.551229	1147.551083	4.976909	-0.013641	1.951876
68.865259	1155.690986	4.981914	-0.013705	1.957804
68.888210	1163.805435	4.986918	-0.013715	1.963665
69.270923	1171.917975	4.991923	-0.013791	1.969545
69.478552	1180.047694	4.996928	-0.013836	1.975401
69.906947	1188.123374	5.001933	-0.013921	1.981225
70.379793	1196.208469	5.006938	-0.014015	1.987043
70.589138	1204.347409	5.011942	-0.014059	1.992854
70.583030	1212.500858	5.016947	-0.014064	1.998636
70.868554	1220.575883	5.021952	-0.014122	2.004377
71.000631	1228.702583	5.026957	-0.014152	2.010121
71.281948	1236.813688	5.031962	-0.014210	2.015854
71.615074	1244.883402	5.036966	-0.014278	2.021546
72.138678	1252.963482	5.041971	-0.014381	2.027249
72.245134	1261.121492	5.046976	-0.014406	2.032948
72.684198	1269.197127	5.051981	-0.014494	2.038607
72.977127	1277.282326	5.056986	-0.014554	2.044243
73.161658	1285.384971	5.061990	-0.014594	2.049864
73.634290	1293.477099	5.066995	-0.014687	2.055491
74.005141	1301.558273	5.072000	-0.014762	2.061085
74.205378	1309.668414	5.077005	-0.014805	2.066666
74.563101	1317.774473	5.082010	-0.014877	2.072246
74.775690	1325.886706	5.087014	-0.014922	2.077800
75.282301	1333.952527	5.092019	-0.015022	2.083336
75.518573	1342.051637	5.097024	-0.015071	2.088854
75.662289	1350.187650	5.102029	-0.015104	2.094373
75.899228	1358.277772	5.107034	-0.015153	2.099856
76.052656	1366.363477	5.112038	-0.015187	2.105313
76.611886	1374.461223	5.117043	-0.015297	2.110804
77.159025	1382.564974	5.122048	-0.015405	2.116283
77.372371	1390.625483	5.127053	-0.015450	2.121687
77.403805	1398.750746	5.132058	-0.015461	2.127102
77.712463	1406.819965	5.137062	-0.015524	2.132493
78.070014	1414.902126	5.142067	-0.015596	2.137884
78.380871	1422.966513	5.147072	-0.015660	2.143245
78.457871	1431.076534	5.152077	-0.015680	2.148600
78.738273	1439.194885	5.157082	-0.015737	2.153967
78.834175	1447.276926	5.162086	-0.015761	2.159279
79.359387	1455.318449	5.167091	-0.015864	2.164591
79.643166	1463.409492	5.172096	-0.015922	2.169900
79.669780	1471.525239	5.177101	-0.015933	2.175189
79.945482	1479.612888	5.182106	-0.015990	2.180469
80.151992	1487.682191	5.187110	-0.016034	2.185719
80.582523	1495.774379	5.192115	-0.016120	2.190991
80.752460	1503.886905	5.197120	-0.016157	2.196239
81.016454	1511.938176	5.202125	-0.016211	2.201444
81.436606	1519.997882	5.207130	-0.016295	2.206657
81.673089	1528.079898	5.212134	-0.016345	2.211854
81.953164	1536.171800	5.217139	-0.016402	2.217050
82.193811	1544.231561	5.222144	-0.016453	2.222209
82.264546	1552.333583	5.227149	-0.016471	2.227369
82.570870	1560.436975	5.232154	-0.016534	2.232537
82.682638	1568.505372	5.237158	-0.016560	2.237655
82.898587	1576.574567	5.242163	-0.016606	2.242771
83.302440	1584.616552	5.247168	-0.016687	2.247874
83.521018	1592.722308	5.252173	-0.016733	2.252989
83.635047	1600.818346	5.257178	-0.016760	2.258078
84.025702	1608.843632	5.262182	-0.016838	2.263135
84.315186	1616.930719	5.267187	-0.016898	2.268210
84.401070	1625.111239	5.272192	-0.016919	2.273314
84.453245	1633.169586	5.277197	-0.016934	2.278329
84.892242	1641.187778	5.282202	-0.017022	2.283340
85.024337	1649.247293	5.287206	-0.017052	2.288340
85.385367	1657.316291	5.292211	-0.017125	2.293354
85.718213	1665.364739	5.297216	-0.017192	2.298342
85.776445	1673.442195	5.302221	-0.017208	2.303314
86.068817	1681.518295	5.307226	-0.017268	2.308294
86.093250	1689.624747	5.312230	-0.017278	2.313259
86.465612	1697.659377	5.317235	-0.017353	2.318199
86.484086	1705.746917	5.322240	-0.017362	2.323131
86.880827	1713.779286	5.327245	-0.017442	2.328050
87.006576	1721.896973	5.332250	-0.017471	2.332988
87.071084	1729.968311	5.337254	-0.017488	2.337883
87.269316	1738.032003	5.342259	-0.017531	2.342774
87.600799	1746.086339	5.347264	-0.017598	2.347659
87.773029	1754.178210	5.352269	-0.017635	2.352545
87.779166	1762.274364	5.357274	-0.017642	2.357409
88.133513	1770.282126	5.362278	-0.017714	2.362238
88.242314	1778.355814	5.367283	-0.017739	2.367077
88.480562	1786.421882	5.372288	-0.017789	2.371912
88.762816	1794.475060	5.377293	-0.017847	2.376733
89.131957	1802.516835	5.382298	-0.017922	2.381544
89.067254	1810.611147	5.387302	-0.017915	2.386342
89.279214	1818.695253	5.392307	-0.017960	2.391146
89.530882	1826.752128	5.397312	-0.018013	2.395928
89.710199	1834.793071	5.402317	-0.018051	2.400685
89.969111	1842.855416	5.407322	-0.018105	2.405451
90.331461	1850.893310	5.412326	-0.018178	2.410202
90.488565	1859.004690	5.417331	-0.018213	2.414970
90.769924	1867.055387	5.422336	-0.018271	2.419703
91.018954	1875.089135	5.427341	-0.018323	2.424414
91.397630	1883.166842	5.432346	-0.018399	2.429152
91.360476	1891.335631	5.437350	-0.018397	2.433901
91.434826	1899.383213	5.442355	-0.018417	2.438580
91.851893	1907.377460	5.447360	-0.018500	2.443244
91.906039	1915.432272	5.452365	-0.018516	2.447907
91.992197	1923.534556	5.457370	-0.018537	2.452591
92.176882	1931.574399	5.462374	-0.018577	2.457238
92.469693	1939.611089	5.467379	-0.018637	2.461882
92.792132	1947.642676	5.472384	-0.018703	2.466516
92.899813	1955.720336	5.477389	-0.018728	2.471152
93.468751	1963.768994	5.482394	-0.018840	2.475797
93.782967	1971.784703	5.487398	-0.018904	2.480396
93.708739	1979.887074	5.492403	-0.018895	2.485006
93.831383	1987.959688	5.497408	-0.018924	2.489606
94.184659	1996.003961	5.502413	-0.018995	2.494198
94.448313	2004.071849	5.507418	-0.019050	2.498788
94.636241	2012.106230	5.512422	-0.019090	2.503345
94.824422	2020.187732	5.517427	-0.019131	2.507921
95.120550	2028.266621	5.522432	-0.019191	2.512495
95.226220	2036.327401	5.527437	-0.019217	2.517036
95.480508	2044.387918	5.532442	-0.019269	2.521580
95.361822	2052.441234	5.537446	-0.019253	2.526084
95.559402	2060.500237	5.542451	-0.019295	2.530606
95.980095	2068.532693	5.547456	-0.019379	2.535122
95.988132	2076.585570	5.552461	-0.019386	2.539611
96.202947	2084.647434	5.557466	-0.019432	2.544112
96.462389	2092.672472	5.562470	-0.019485	2.548588
96.745439	2100.733869	5.567475	-0.019544	2.553077
96.961031	2108.787141	5.572480	-0.019589	2.557550
97.172319	2116.820131	5.577485	-0.019634	2.562003
97.369706	2124.895055	5.582490	-0.019676	2.566470
97.442093	2132.964767	5.587494	-0.019695	2.570918
97.577395	2141.043708	5.592499	-0.019726	2.575368
97.657200	2149.095573	5.597504	-0.019747	2.579792
97.767205	2157.124720	5.602509	-0.019773	2.584197
98.291666	2165.171382	5.607514	-0.019876	2.588633
98.319300	2173.379397	5.612518	-0.019886	2.593115
98.538871	2181.425971	5.617523	-0.019933	2.597515
98.893050	2189.397439	5.622528	-0.020004	2.601875
98.924791	2197.433331	5.627533	-0.020016	2.606242
99.369578	2205.456977	5.632538	-0.020104	2.610622
99.479843	2213.501587	5.637542	-0.020130	2.614983
99.678620	2221.521834	5.642547	-0.020173	2.619331
100.163117	2229.530571	5.647552	-0.020268	2.623683
100.485935	2237.566227	5.652557	-0.020334	2.628032
100.595619	2245.679777	5.657562	-0.020360	2.632402
100.951824	2253.686266	5.662566	-0.020432	2.636723
101.138046	2261.736067	5.667571	-0.020472	2.641049
101.360725	2269.796750	5.672576	-0.020519	2.645376
101.296776	2277.851533	5.677581	-0.020512	2.649674
101.602927	2285.922081	5.682586	-0.020575	2.653998
101.635422	2293.963149	5.687590	-0.020587	2.658281
102.043616	2301.988977	5.692595	-0.020668	2.662573
102.219092	2310.047543	5.697600	-0.020706	2.666861
102.409790	2318.113799	5.702605	-0.020747	2.671147
102.783408	2326.193943	5.707610	-0.020822	2.675445
102.947642	2334.197338	5.712614	-0.020858	2.679682
103.178162	2342.233328	5.717619	-0.020907	2.683934
103.194289	2350.314066	5.722624	-0.020915	2.688189
103.231810	2358.371158	5.727629	-0.020928	2.692426
103.656618	2366.403222	5.732634	-0.021013	2.696668
103.943206	2374.423078	5.737638	-0.021071	2.700888
104.040831	2382.467604	5.742643	-0.021095	2.705103
104.319098	2390.518626	5.747648	-0.021152	2.709325
104.617690	2398.578146	5.752653	-0.021214	2.713547
104.678029	2406.654281	5.757658	-0.021230	2.717755
104.727477	2414.668552	5.762662	-0.021245	2.721925
105.313482	2422.685981	5.767667	-0.021360	2.726123
105.615007	2430.738507	5.772672	-0.021421	2.730315
105.611822	2438.831330	5.777677	-0.021426	2.734502
105.720029	2446.880421	5.782682	-0.021452	2.738668
106.180903	2454.869801	5.787686	-0.021543	2.742817
106.299806	2462.942908	5.792691	-0.021571	2.746983
106.320201	2471.046652	5.797696	-0.021580	2.751152
106.692959	2479.121808	5.802701	-0.021655	2.755322
107.150435	2487.090381	5.807706	-0.021746	2.759435
107.171182	2495.127273	5.812710	-0.021755	2.763551
107.592216	2503.133524	5.817715	-0.021839	2.767669
107.732109	2511.201373	5.822720	-0.021871	2.771796
107.627293	2519.266400	5.827725	-0.021857	2.775901
107.853144	2527.311499	5.832730	-0.021904	2.780008
108.171628	2535.305590	5.837734	-0.021969	2.784090
108.231410	2543.368762	5.842739	-0.021986	2.788185
108.482758	2551.441948	5.847744	-0.022038	2.792290
108.781083	2559.458118	5.852749	-0.022099	2.796364
109.051003	2567.498713	5.857754	-0.022155	2.800442
108.889495	2575.529781	5.862758	-0.022130	2.804484
109.174166	2583.581083	5.867763	-0.022189	2.808556
109.506545	2591.620736	5.872768	-0.022256	2.812619
109.486295	2599.690326	5.877773	-0.022258	2.816671
109.780200	2607.726784	5.882778	-0.022318	2.820719
109.841810	2615.742914	5.887782	-0.022335	2.824737
110.161312	2623.790377	5.892787	-0.022400	2.828780
110.353791	2631.897815	5.897792	-0.022441	2.832840
110.414688	2639.930493	5.902797	-0.022458	2.836850
110.730773	2647.947442	5.907802	-0.022523	2.840860
110.882453	2655.941160	5.912806	-0.022556	2.844843
111.397898	2663.949622	5.917811	-0.022658	2.848849
111.730331	2672.018704	5.922816	-0.022725	2.852869
111.592735	2680.100703	5.927821	-0.022705	2.856863
111.928354	2688.124169	5.932826	-0.022773	2.860850
112.187683	2696.132805	5.937830	-0.022827	2.864819
112.340645	2704.194426	5.942835	-0.022861	2.868802
112.675731	2712.257704	5.947840	-0.022929	2.872791
112.898912	2720.264856	5.952845	-0.022976	2.876741
113.054335	2728.319345	5.957850	-0.023010	2.880705
113.257984	2736.322937	5.962854	-0.023054	2.884641
113.367955	2744.392033	5.967859	-0.023080	2.888598
113.762098	2752.442585	5.972864	-0.023159	2.892556
113.967963	2760.479222	5.977869	-0.023203	2.896492
114.177301	2768.530370	5.982874	-0.023247	2.900430
114.289558	2776.544942	5.987878	-0.023273	2.904339
114.471886	2784.614676	5.992883	-0.023313	2.908274
114.646853	2792.729061	5.997888	-0.023351	2.912225
114.724257	2800.791229	6.002893	-0.023371	2.916139
114.836712	2808.794001	6.007898	-0.023397	2.920022
114.845198	2816.789828	6.012902	-0.023404	2.923890
115.203063	2824.808466	6.017907	-0.023477	2.927783
115.364458	2832.848429	6.022912	-0.023512	2.931671
115.762803	2840.862299	6.027917	-0.023592	2.935553
115.949472	2848.897053	6.032922	-0.023632	2.939429
116.002012	2856.944740	6.037926	-0.023647	2.943299
116.251106	2864.977181	6.042931	-0.023699	2.947167
116.482527	2873.028748	6.047936	-0.023748	2.951038
116.793025	2881.058975	6.052941	-0.023811	2.954897
117.009385	2889.091077	6.057946	-0.023857	2.958748
117.048054	2897.127376	6.062950	-0.023870	2.962587
117.233150	2905.143317	6.067955	-0.023910	2.966418
117.568277	2913.198904	6.072960	-0.023978	2.970271
117.825055	2921.243962	6.077965	-0.024031	2.974110
117.957267	2929.287220	6.082970	-0.024061	2.977936
118.171329	2937.298577	6.087974	-0.024106	2.981747
118.418070	2945.344521	6.092979	-0.024158	2.985571
118.619354	2953.383960	6.097984	-0.024201	2.989384
118.707446	2961.476205	6.102989	-0.024223	2.993212
118.991133	2969.497900	6.107994	-0.024281	2.997012
119.112158	2977.500065	6.112998	-0.024309	3.000789
119.536875	2985.471706	6.118003	-0.024394	3.004562
119.703011	2993.553273	6.123008	-0.024430	3.008370
119.666002	3001.605313	6.128013	-0.024429	3.012148
119.925494	3009.664986	6.133018	-0.024483	3.015940
120.018649	3017.672987	6.138022	-0.024505	3.019695
120.124534	3025.719068	6.143027	-0.024531	3.023464
120.311609	3033.757416	6.148032	-0.024571	3.027228
121.063574	3041.743016	6.153037	-0.024717	3.030990
121.564058	3049.796593	6.158042	-0.024815	3.034767
121.684047	3057.821420	6.163046	-0.024843	3.038508
121.926533	3065.855614	6.168051	-0.024894	3.042254
122.231076	3073.888045	6.173056	-0.024956	3.045997
122.475481	3081.923928	6.178061	-0.025007	3.049735
122.835275	3090.001768	6.183066	-0.025079	3.053493
122.689267	3098.050567	6.188070	-0.025058	3.057209
122.826959	3106.092154	6.193075	-0.025089	3.060930
123.270698	3114.078412	6.198080	-0.025177	3.064636
123.303984	3122.129406	6.203085	-0.025189	3.068348
123.453219	3130.241465	6.208090	-0.025222	3.072088
124.114018	3138.255687	6.213094	-0.025351	3.075804
124.437759	3146.222349	6.218099	-0.025416	3.079477
124.731972	3154.249374	6.223104	-0.025477	3.083172
124.824751	3162.275206	6.228109	-0.025499	3.086852
125.190034	3170.307719	6.233114	-0.025573	3.090544
125.206411	3178.357872	6.238118	-0.025582	3.094223
125.682199	3186.375490	6.243123	-0.025676	3.097904
125.858980	3194.428134	6.248128	-0.025714	3.101583
125.705237	3202.463887	6.253133	-0.025691	3.105235
126.255655	3210.499012	6.258138	-0.025799	3.108914
126.229130	3218.557551	6.263142	-0.025800	3.112574
126.289966	3226.611351	6.268147	-0.025816	3.116230
126.485476	3234.608863	6.273152	-0.025858	3.119863
126.875739	3242.596466	6.278157	-0.025936	3.123497
127.078313	3250.663995	6.283162	-0.025980	3.127153
127.168415	3258.702393	6.288166	-0.026002	3.130787
127.343750	3266.745234	6.293171	-0.026040	3.134423
127.542706	3274.802115	6.298176	-0.026083	3.138061
127.681920	3282.791029	6.303181	-0.026114	3.141663
128.145734	3290.816410	6.308186	-0.026206	3.145290
128.182930	3298.861763	6.313190	-0.026218	3.148904
128.403131	3306.922881	6.318195	-0.026265	3.152529
128.857721	3314.967745	6.323200	-0.026355	3.156152
128.967937	3322.940408	6.328205	-0.026381	3.159724
129.072741	3330.984891	6.333210	-0.026406	3.163324
129.280604	3339.000613	6.338214	-0.026450	3.166911
129.487759	3347.043119	6.343219	-0.026494	3.170506
129.702073	3355.120827	6.348224	-0.026540	3.174113
129.674077	3363.139201	6.353229	-0.026540	3.177679
129.792396	3371.188356	6.358234	-0.026568	3.181260
129.914123	3379.173131	6.363238	-0.026596	3.184810
130.053139	3387.233568	6.368243	-0.026627	3.188390
130.183685	3395.262334	6.373248	-0.026657	3.191951
130.557329	3403.293896	6.378253	-0.026732	3.195520
130.732091	3411.313268	6.383258	-0.026770	3.199071
130.889168	3419.322094	6.388262	-0.026805	3.202612
131.203530	3427.348338	6.393267	-0.026869	3.206164
131.408816	3435.378362	6.398272	-0.026913	3.209709
131.295285	3443.459547	6.403277	-0.026897	3.213259
131.593428	3451.486662	6.408282	-0.026958	3.216799
131.822383	3459.475905	6.413286	-0.027006	3.220315
131.893925	3467.502308	6.418291	-0.027025	3.223838
132.121224	3475.564313	6.423296	-0.027073	3.227378
132.378310	3483.596092	6.428301	-0.027126	3.230902
132.538620	3491.706558	6.433306	-0.027162	3.234453
132.732850	3499.680468	6.438310	-0.027203	3.237942
133.057720	3507.668858	6.443315	-0.027269	3.241439
133.234393	3515.681208	6.448320	-0.027308	3.244936
133.412990	3523.679144	6.453325	-0.027346	3.248423
133.785791	3531.741873	6.458330	-0.027421	3.251943
134.004576	3539.796053	6.463334	-0.027467	3.255449
133.957316	3547.809292	6.468339	-0.027464	3.258922
134.294274	3555.847026	6.473344	-0.027532	3.262418
134.477313	3563.889592	6.478349	-0.027572	3.265906
134.787820	3571.890918	6.483354	-0.027635	3.269377
134.855089	3579.959236	6.488358	-0.027653	3.272864
135.253919	3588.003158	6.493363	-0.027733	3.276350
135.522117	3595.996662	6.498368	-0.027789	3.279805
135.724179	3603.989480	6.503373	-0.027832	3.283253
136.077459	3612.030903	6.508378	-0.027903	3.286725
135.887260	3620.089270	6.513382	-0.027873	3.290179
136.199535	3628.131940	6.518387	-0.027937	3.293643
136.391279	3636.164903	6.523392	-0.027978	3.297093
136.435842	3644.175063	6.528397	-0.027992	3.300525
136.800416	3652.178138	6.533402	-0.028065	3.303962
136.900397	3660.211860	6.538406	-0.028089	3.307399
137.193758	3668.231668	6.543411	-0.028149	3.310834
137.473238	3676.313927	6.548416	-0.028207	3.314291
137.507880	3684.317926	6.553421	-0.028219	3.317701
137.929521	3692.341493	6.558426	-0.028303	3.321131
137.944995	3700.354273	6.563430	-0.028311	3.324538
138.020637	3708.395738	6.568435	-0.028331	3.327956
138.436544	3716.422265	6.573440	-0.028414	3.331376
138.516406	3724.459415	6.578445	-0.028434	3.334785
138.850237	3732.492229	6.583450	-0.028502	3.338198
138.951875	3740.516750	6.588454	-0.028526	3.341596
138.967526	3748.516311	6.593459	-0.028535	3.344976
139.365774	3756.558111	6.598464	-0.028614	3.348384
139.291264	3764.617400	6.603469	-0.028606	3.351780
139.357517	3772.710490	6.608474	-0.028624	3.355191
139.537881	3780.682491	6.613478	-0.028663	3.358552
139.864171	3788.680482	6.618483	-0.028729	3.361925
140.291689	3796.698063	6.623488	-0.028814	3.365307
140.464400	3804.730854	6.628493	-0.028852	3.368683
140.762092	3812.811799	6.633498	-0.028913	3.372080
140.735847	3820.846587	6.638502	-0.028913	3.375443
141.138591	3828.801353	6.643507	-0.028994	3.378784
141.378886	3836.843770	6.648512	-0.029044	3.382153
141.284342	3844.886011	6.653517	-0.029032	3.385506
141.615343	3852.915218	6.658522	-0.029099	3.388866
141.841499	3861.004138	6.663526	-0.029147	3.392243
142.149005	3869.043351	6.668531	-0.029210	3.395599
142.131916	3877.036757	6.673536	-0.029212	3.398922
142.260891	3885.009211	6.678541	-0.029241	3.402237
142.657345	3893.020623	6.683546	-0.029321	3.405575
142.645397	3901.042467	6.688550	-0.029324	3.408899
142.761827	3909.099942	6.693555	-0.029351	3.412240
142.994386	3917.159521	6.698560	-0.029400	3.415582
143.155751	3925.133235	6.703565	-0.029436	3.418883
143.372247	3933.179033	6.708570	-0.029481	3.422212
143.485916	3941.186719	6.713574	-0.029508	3.425519
143.630458	3949.198908	6.718579	-0.029540	3.428826
144.089518	3957.253831	6.723584	-0.029631	3.432157
144.108305	3965.323180	6.728589	-0.029640	3.435476
144.378811	3973.300755	6.733594	-0.029696	3.438763
144.513961	3981.338963	6.738598	-0.029727	3.442067
144.771772	3989.332353	6.743603	-0.029780	3.445354
145.174080	3997.370597	6.748608	-0.029861	3.448660
145.339432	4005.425210	6.753613	-0.029897	3.451962
145.453217	4013.497125	6.758618	-0.029924	3.455267
145.632849	4021.487424	6.763622	-0.029963	3.458537
145.923271	4029.512462	6.768627	-0.030022	3.461821
145.963768	4037.527723	6.773632	-0.030035	3.465091
146.055917	4045.572529	6.778637	-0.030058	3.468371
146.274399	4053.631060	6.783642	-0.030104	3.471657
146.423381	4061.654457	6.788646	-0.030138	3.474924
146.521899	4069.634881	6.793651	-0.030161	3.478169
146.866467	4077.676486	6.798656	-0.030231	3.481443
146.974572	4085.645855	6.803661	-0.030257	3.484678
147.235101	4093.682416	6.808666	-0.030311	3.487941
147.406782	4101.721252	6.813670	-0.030348	3.491199
147.569886	4109.744406	6.818675	-0.030384	3.494448
147.803070	4117.786653	6.823680	-0.030433	3.497704
147.803570	4125.803538	6.828685	-0.030438	3.500939
148.019224	4133.816558	6.833690	-0.030484	3.504176
148.369467	4141.846055	6.838694	-0.030555	3.507421
148.487707	4149.865381	6.843699	-0.030582	3.510652
148.549712	4157.940776	6.848704	-0.030599	3.513900
148.798725	4165.925314	6.853709	-0.030651	3.517115
148.860169	4173.977590	6.858714	-0.030668	3.520348
148.949269	4181.958059	6.863718	-0.030690	3.523550
149.404259	4189.985756	6.868723	-0.030780	3.526780
149.622456	4198.032028	6.873728	-0.030827	3.530006
149.647041	4206.057501	6.878733	-0.030837	3.533216
150.042315	4214.106790	6.883738	-0.030916	3.536443
150.274954	4222.091377	6.888742	-0.030965	3.539636
150.375839	4230.136300	6.893747	-0.030989	3.542847
150.631918	4238.175345	6.898752	-0.031042	3.546057
150.822529	4246.195314	6.903757	-0.031083	3.549255
151.143142	4254.318153	6.908762	-0.031148	3.552494
151.128273	4262.369789	6.913766	-0.031151	3.555692
151.439099	4270.306088	6.918771	-0.031214	3.558851
151.674237	4278.321363	6.923776	-0.031264	3.562037
151.625973	4286.318378	6.928781	-0.031260	3.565204
152.251102	4294.317784	6.933786	-0.031382	3.568389
152.287084	4302.395623	6.938790	-0.031394	3.571584
152.570837	4310.413527	6.943795	-0.031453	3.574761
152.704781	4318.425929	6.948800	-0.031483	3.577927
152.965825	4326.423549	6.953805	-0.031537	3.581089
153.332636	4334.408774	6.958810	-0.031611	3.584247
153.439082	4342.451851	6.963814	-0.031636	3.587416
153.787353	4350.490938	6.968819	-0.031707	3.590589
154.010268	4358.543970	6.973824	-0.031754	3.593760
153.844396	4366.560638	6.978829	-0.031728	3.596903
154.100794	4374.557103	6.983834	-0.031781	3.600048
154.385353	4382.561854	6.988838	-0.031840	3.603194
154.466272	4390.600247	6.993843	-0.031861	3.606344
154.664537	4398.607818	6.998848	-0.031903	3.609483
154.725779	4406.650568	7.003853	-0.031920	3.612629
155.181384	4414.693211	7.008858	-0.032010	3.615783
155.074549	4422.714006	7.013862	-0.031996	3.618910
155.338866	4430.734768	7.018867	-0.032051	3.622045
155.517585	4438.761405	7.023872	-0.032089	3.625177
155.671994	4446.772704	7.028877	-0.032124	3.628300
155.866687	4454.838761	7.033882	-0.032165	3.631442
156.168910	4462.864217	7.038886	-0.032227	3.634569
156.366635	4470.902380	7.043891	-0.032269	3.637695
156.566245	4478.929709	7.048896	-0.032312	3.640814
156.597330	4486.887017	7.053901	-0.032323	3.643899
156.653685	4494.982433	7.058906	-0.032339	3.647035
156.764490	4503.000383	7.063910	-0.032366	3.650140
156.994784	4511.025917	7.068915	-0.032414	3.653249
157.154963	4519.080170	7.073920	-0.032449	3.656364
157.182292	4527.033068	7.078925	-0.032460	3.659434
157.322311	4535.049810	7.083930	-0.032491	3.662529
157.453759	4543.094251	7.088934	-0.032521	3.665631
157.613805	4551.126603	7.093939	-0.032557	3.668727
157.699727	4559.176496	7.098944	-0.032578	3.671826
157.954397	4567.176387	7.103949	-0.032631	3.674907
158.225045	4575.169839	7.108954	-0.032687	3.677983
158.392978	4583.198137	7.113958	-0.032724	3.681067
158.265234	4591.193454	7.118963	-0.032705	3.684128
158.593253	4599.266241	7.123968	-0.032772	3.687228
158.727715	4607.250232	7.128973	-0.032803	3.690287
159.202639	4615.271544	7.133978	-0.032896	3.693366
159.374624	4623.298444	7.138982	-0.032934	3.696437
159.460363	4631.310758	7.143987	-0.032955	3.699497
159.422835	4639.354194	7.148992	-0.032954	3.702564
159.708873	4647.355322	7.153997	-0.033013	3.705620
160.037627	4655.379279	7.159002	-0.033079	3.708684
160.056903	4663.462104	7.164006	-0.033089	3.711759
160.190747	4671.544245	7.169011	-0.033119	3.714834
160.701872	4679.506870	7.174016	-0.033220	3.717871
160.742926	4687.494090	7.179021	-0.033233	3.720903
160.913294	4695.500161	7.184026	-0.033270	3.723943
161.104435	4703.529666	7.189030	-0.033311	3.726990
161.348235	4711.532780	7.194035	-0.033362	3.730026
161.718917	4719.568332	7.199040	-0.033436	3.733074
161.810736	4727.610085	7.204045	-0.033459	3.736115
162.212505	4735.577685	7.209050	-0.033539	3.739134
162.183078	4743.619581	7.214054	-0.033539	3.742167
162.337187	4751.656492	7.219059	-0.033574	3.745201
162.730052	4759.694196	7.224064	-0.033652	3.748238
162.727323	4767.724243	7.229069	-0.033657	3.751260
162.671963	4775.772345	7.234074	-0.033652	3.754286
163.102576	4783.777724	7.239078	-0.033738	3.757304
163.386426	4791.771343	7.244083	-0.033796	3.760312
163.762421	4799.782477	7.249088	-0.033872	3.763327
163.988289	4807.792749	7.254093	-0.033919	3.766335
164.133097	4815.841169	7.259098	-0.033952	3.769353
164.092156	4823.924118	7.264102	-0.033950	3.772377
164.360484	4831.917924	7.269107	-0.034005	3.775373
164.726966	4839.907248	7.274112	-0.034079	3.778366
164.724998	4847.970480	7.279117	-0.034084	3.781377
164.830246	4855.944120	7.284122	-0.034109	3.784354
165.296218	4864.015572	7.289126	-0.034202	3.787373
165.483475	4872.020612	7.294131	-0.034242	3.790359
165.466924	4880.122237	7.299136	-0.034244	3.793374
165.466554	4888.136965	7.304141	-0.034250	3.796355
165.622528	4896.094115	7.309146	-0.034284	3.799315
165.785873	4904.085711	7.314150	-0.034320	3.802286
165.968475	4912.047146	7.319155	-0.034360	3.805244
166.395406	4920.112597	7.324160	-0.034445	3.808243
166.618457	4928.141703	7.329165	-0.034492	3.811222
166.845283	4936.177819	7.334170	-0.034539	3.814201
167.020168	4944.192092	7.339174	-0.034577	3.817169
167.037634	4952.226858	7.344179	-0.034586	3.820139
167.128229	4960.236612	7.349184	-0.034609	3.823098
167.219530	4968.272894	7.354189	-0.034631	3.826066
167.592563	4976.254441	7.359194	-0.034706	3.829016
167.548478	4984.318666	7.364198	-0.034703	3.831986
167.693371	4992.305430	7.369203	-0.034736	3.834929
167.980577	5000.339585	7.374208	-0.034795	3.837890
168.059286	5008.317069	7.379213	-0.034815	3.840824
168.311155	5016.335173	7.384218	-0.034867	3.843774
168.422729	5024.369121	7.389222	-0.034894	3.846725
168.766737	5032.364794	7.394227	-0.034963	3.849664
168.759037	5040.501386	7.399232	-0.034967	3.852645
168.795990	5048.492527	7.404237	-0.034980	3.855572
169.045830	5056.521531	7.409242	-0.035032	3.858514
169.150959	5064.536558	7.414246	-0.035057	3.861446
169.076591	5072.510300	7.419251	-0.035048	3.864357
169.377453	5080.606407	7.424256	-0.035110	3.867319
169.431003	5088.605025	7.429261	-0.035125	3.870237
169.561960	5096.812032	7.434266	-0.035155	3.873231
169.793154	5104.850222	7.439270	-0.035204	3.876163
169.978266	5112.738311	7.444275	-0.035244	3.879037
170.154554	5120.729866	7.449280	-0.035282	3.881946
170.199521	5128.665765	7.454285	-0.035296	3.884831
170.617775	5136.728750	7.459290	-0.035379	3.887766
170.808332	5144.748998	7.464294	-0.035420	3.890680
170.671285	5152.771156	7.469299	-0.035400	3.893585
171.077195	5160.820617	7.474304	-0.035481	3.896509
171.216396	5168.772120	7.479309	-0.035513	3.899390
171.172962	5176.852245	7.484314	-0.035510	3.902312
171.449920	5184.831835	7.489318	-0.035567	3.905201
171.592881	5192.853827	7.494323	-0.035599	3.908101
171.875106	5200.892808	7.499328	-0.035657	3.911008
171.727174	5208.926313	7.504333	-0.035635	3.913902
171.902138	5216.962982	7.509338	-0.035673	3.916802
172.095991	5224.891104	7.514342	-0.035715	3.919660
172.038947	5232.948997	7.519347	-0.035710	3.922559
172.273528	5240.962404	7.524352	-0.035759	3.925444
172.441812	5248.976478	7.529357	-0.035796	3.928327
172.625923	5257.049653	7.534362	-0.035836	3.931229
172.897564	5265.066159	7.539366	-0.035892	3.934110
172.780195	5273.057600	7.544371	-0.035875	3.936973
172.864385	5281.048257	7.549376	-0.035897	3.939837
173.042517	5289.085475	7.554381	-0.035935	3.942717
173.416645	5297.091024	7.559386	-0.036010	3.945588
173.453239	5305.113953	7.564390	-0.036023	3.948456
173.389644	5313.145906	7.569395	-0.036016	3.951324
173.607210	5321.218935	7.574400	-0.036062	3.954209
173.733388	5329.215722	7.579405	-0.036091	3.957064
173.783754	5337.203617	7.584410	-0.036106	3.959912
174.047637	5345.198383	7.589414	-0.036161	3.962764
174.182908	5353.194681	7.594419	-0.036192	3.965612
174.350054	5361.238297	7.599424	-0.036228	3.968475
174.343887	5369.266190	7.604429	-0.036233	3.971328
174.518695	5377.317646	7.609434	-0.036271	3.974190
174.680000	5385.360666	7.614438	-0.036306	3.977047
174.800001	5393.356006	7.619443	-0.036334	3.979885
175.045953	5401.361777	7.624448	-0.036385	3.982726
175.033713	5409.358099	7.629453	-0.036388	3.985557
175.402619	5417.411218	7.634458	-0.036463	3.988413
175.425221	5425.460706	7.639462	-0.036472	3.991259
175.636835	5433.478951	7.644467	-0.036517	3.994096
175.967756	5441.516087	7.649472	-0.036584	3.996939
175.829080	5449.494720	7.654477	-0.036564	3.999752
176.074958	5457.536690	7.659482	-0.036615	4.002592
176.148131	5465.557747	7.664486	-0.036634	4.005419
176.266599	5473.560287	7.669491	-0.036662	4.008238
176.637284	5481.598897	7.674496	-0.036737	4.011073
176.672655	5489.619287	7.679501	-0.036749	4.013893
177.059770	5497.645658	7.684506	-0.036826	4.016719
177.030678	5505.636729	7.689510	-0.036826	4.019524
177.187661	5513.638506	7.694515	-0.036861	4.022334
177.294600	5521.682896	7.699520	-0.036886	4.025156
177.438754	5529.697479	7.704525	-0.036919	4.027966
177.678526	5537.735858	7.709530	-0.036969	4.030784
177.971377	5545.886576	7.714534	-0.037029	4.033640
178.168376	5553.840094	7.719539	-0.037071	4.036424
178.380197	5561.777098	7.724544	-0.037116	4.039200
178.273339	5569.796824	7.729549	-0.037102	4.041998
178.622704	5577.796350	7.734554	-0.037172	4.044794
178.824642	5585.843656	7.739558	-0.037215	4.047603
178.907304	5593.825487	7.744563	-0.037236	4.050385
178.942030	5601.899186	7.749568	-0.037248	4.053196
179.029598	5609.924237	7.754573	-0.037270	4.055989
179.204900	5617.901801	7.759578	-0.037308	4.058765
179.363967	5625.955697	7.764582	-0.037343	4.061566
179.726295	5633.859310	7.769587	-0.037416	4.064315
179.729973	5641.971302	7.774592	-0.037422	4.067129
179.776603	5649.944842	7.779597	-0.037436	4.069895
180.129338	5658.003318	7.784602	-0.037508	4.072692
180.091650	5666.043612	7.789606	-0.037506	4.075475
180.366977	5674.006372	7.794611	-0.037563	4.078234
180.744436	5682.048229	7.799616	-0.037639	4.081020
180.762946	5690.024207	7.804621	-0.037648	4.083776
180.832714	5698.071389	7.809626	-0.037666	4.086555
180.918654	5706.070951	7.814630	-0.037688	4.089317
181.099916	5714.108443	7.819635	-0.037727	4.092090
181.136793	5722.162562	7.824640	-0.037739	4.094866
181.053185	5730.167909	7.829645	-0.037729	4.097622
181.306824	5738.185515	7.834650	-0.037782	4.100384
181.470581	5746.186678	7.839654	-0.037818	4.103138
181.541284	5754.205949	7.844659	-0.037837	4.105894
181.769537	5762.261010	7.849664	-0.037885	4.108664
181.784413	5770.309690	7.854669	-0.037893	4.111426
182.122348	5778.341576	7.859674	-0.037961	4.114185
182.137119	5786.356519	7.864678	-0.037969	4.116932
182.334486	5794.298875	7.869683	-0.038012	4.119655
182.551626	5802.328876	7.874688	-0.038058	4.122406
182.530911	5810.336615	7.879693	-0.038059	4.125144
182.691279	5818.359457	7.884698	-0.038095	4.127889
182.608986	5826.423111	7.889702	-0.038085	4.130642
182.886690	5834.428688	7.894707	-0.038142	4.133378
183.327328	5842.485062	7.899712	-0.038230	4.136132
183.450526	5850.461318	7.904717	-0.038258	4.138852
183.518688	5858.484274	7.909722	-0.038276	4.141586
183.559814	5866.499770	7.914726	-0.038289	4.144315
183.647815	5874.524421	7.919731	-0.038311	4.147046
183.876237	5882.583445	7.924736	-0.038359	4.149789
183.943703	5890.580928	7.929741	-0.038377	4.152507
184.221435	5898.604871	7.934746	-0.038435	4.155235
184.376246	5906.628345	7.939750	-0.038469	4.157959
184.314649	5914.636061	7.944755	-0.038463	4.160674
184.807241	5922.631837	7.949760	-0.038560	4.163389
184.866830	5930.633967	7.954765	-0.038577	4.166099
185.246249	5938.632348	7.959770	-0.038653	4.168811
185.365148	5946.706749	7.964774	-0.038680	4.171543
185.363796	5954.713832	7.969779	-0.038686	4.174249
185.386845	5962.807600	7.974784	-0.038696	4.176983
185.263155	5970.741300	7.979789	-0.038678	4.179659
185.634440	5978.747075	7.984794	-0.038753	4.182364
185.822705	5986.763255	7.989798	-0.038793	4.185068
185.839406	5994.788432	7.994803	-0.038802	4.187772
186.013838	6002.835046	7.999808	-0.038840	4.190483
186.217404	6010.933357	8.004813	-0.038883	4.193209
186.280619	6018.966275	8.009818	-0.038900	4.195911
186.366868	6026.911654	8.014822	-0.038922	4.198581
186.478553	6034.887373	8.019827	-0.038948	4.201261
186.789380	6042.883398	8.024832	-0.039012	4.203947
186.717625	6050.922672	8.029837	-0.039004	4.206642
186.780519	6058.879042	8.034842	-0.039021	4.209309
186.968910	6066.990486	8.039846	-0.039062	4.212028
186.984812	6074.937114	8.044851	-0.039070	4.214688
187.439146	6082.998696	8.049856	-0.039160	4.217389
187.274997	6090.953519	8.054861	-0.039135	4.220047
187.417138	6098.992918	8.059866	-0.039167	4.222734
187.542594	6107.005261	8.064870	-0.039196	4.225410
187.690263	6115.022085	8.069875	-0.039229	4.228086
187.690223	6123.077438	8.074880	-0.039234	4.230772
187.831722	6131.090668	8.079885	-0.039266	4.233443
188.186177	6139.144110	8.084890	-0.039338	4.236129
188.368963	6147.112981	8.089894	-0.039377	4.238782
188.344792	6155.135112	8.094899	-0.039378	4.241450
188.622442	6163.145250	8.099904	-0.039435	4.244115
188.709619	6171.132076	8.104909	-0.039457	4.246769
188.882118	6179.143186	8.109914	-0.039495	4.249430
189.010623	6187.219930	8.114918	-0.039524	4.252110
189.151443	6195.232724	8.119923	-0.039556	4.254768
189.389396	6203.289400	8.124928	-0.039606	4.257440
189.463792	6211.275531	8.129933	-0.039625	4.260084
189.561353	6219.278305	8.134938	-0.039649	4.262733
189.570243	6227.308321	8.139942	-0.039656	4.265389
189.655426	6235.311077	8.144947	-0.039677	4.268035
189.890968	6243.394283	8.149952	-0.039726	4.270706
190.086650	6251.413689	8.154957	-0.039768	4.273355
190.092818	6259.443106	8.159962	-0.039775	4.276004
190.249896	6267.413920	8.164966	-0.039810	4.278633
190.313801	6275.444239	8.169971	-0.039827	4.281279
190.498341	6283.458460	8.174976	-0.039867	4.283919
190.653355	6291.465168	8.179981	-0.039901	4.286555
190.811355	6299.475851	8.184986	-0.039936	4.289191
191.199280	6307.499102	8.189990	-0.040014	4.291831
191.155919	6315.524819	8.194995	-0.040011	4.294466
191.249119	6323.591113	8.200000	-0.040034	4.297115
191.312699	6331.546051	8.205005	-0.040052	4.299725
191.445098	6339.584213	8.210010	-0.040082	4.302361
191.483243	6347.586731	8.215014	-0.040094	4.304983
191.563849	6355.583605	8.220019	-0.040115	4.307602
191.792986	6363.614332	8.225024	-0.040163	4.310232
191.978658	6371.660630	8.230029	-0.040203	4.312865
192.045056	6379.689850	8.235034	-0.040221	4.315489
192.318500	6387.658995	8.240038	-0.040277	4.318094
192.229605	6395.670035	8.245043	-0.040266	4.320709
192.337962	6403.694841	8.250048	-0.040292	4.323328
192.544773	6411.678295	8.255053	-0.040336	4.325932
192.660132	6419.701271	8.260058	-0.040363	4.328547
192.632836	6427.796551	8.265062	-0.040363	4.331183
192.716685	6435.772462	8.270067	-0.040385	4.333779
192.932509	6443.815635	8.275072	-0.040430	4.336397
193.062727	6451.781049	8.280077	-0.040460	4.338987
193.169676	6459.845030	8.285082	-0.040485	4.341607
193.188140	6467.845574	8.290086	-0.040494	4.344204
193.407084	6475.850590	8.295091	-0.040541	4.346803
193.518074	6483.879096	8.300096	-0.040567	4.349407
193.850660	6491.949369	8.305101	-0.040634	4.352025
194.006191	6500.003162	8.310106	-0.040669	4.354634
194.136857	6507.997710	8.315110	-0.040698	4.357222
194.166570	6515.905434	8.320115	-0.040709	4.359781
194.257520	6523.959583	8.325120	-0.040732	4.362385
194.349734	6531.907409	8.330125	-0.040754	4.364953
194.295612	6539.979812	8.335130	-0.040750	4.367560
194.707907	6547.967787	8.340134	-0.040832	4.370140
194.841503	6556.030805	8.345139	-0.040863	4.372741
194.856268	6564.055373	8.350144	-0.040871	4.375328
195.016170	6572.027725	8.355149	-0.040906	4.377897
195.375686	6580.057435	8.360154	-0.040979	4.380484
195.360261	6588.092049	8.365158	-0.040981	4.383069
195.313573	6596.076613	8.370163	-0.040978	4.385636
195.682201	6604.130383	8.375168	-0.041052	4.388227
195.749899	6612.121424	8.380173	-0.041070	4.390794
195.889564	6620.164574	8.385178	-0.041102	4.393376
195.932370	6628.193739	8.390182	-0.041115	4.395952
196.022697	6636.156700	8.395187	-0.041137	4.398506
196.093202	6644.251367	8.400192	-0.041156	4.401100
196.167455	6652.195726	8.405197	-0.041175	4.403644
196.456541	6660.250483	8.410202	-0.041235	4.406224
196.482481	6668.278220	8.415206	-0.041245	4.408791
196.495257	6676.302074	8.420211	-0.041253	4.411356
196.765216	6684.327525	8.425216	-0.041309	4.413922
196.875261	6692.360256	8.430221	-0.041335	4.416487
196.994356	6700.307535	8.435226	-0.041362	4.419024
197.059979	6708.389505	8.440230	-0.041380	4.421602
197.211048	6716.303481	8.445235	-0.041414	4.424125
197.451822	6724.418741	8.450240	-0.041464	4.426711
197.519226	6732.418774	8.455245	-0.041482	4.429258
197.618839	6740.482853	8.460250	-0.041506	4.431825
197.796461	6748.520099	8.465254	-0.041545	4.434381
197.746214	6756.503358	8.470259	-0.041541	4.436918
198.025571	6764.493489	8.475264	-0.041598	4.439457
198.117520	6772.524322	8.480269	-0.041621	4.442007
198.195036	6780.464529	8.485274	-0.041641	4.444526
198.642697	6788.483156	8.490278	-0.041730	4.447071
198.550646	6796.493913	8.495283	-0.041718	4.449609
198.669762	6804.592279	8.500288	-0.041746	4.452174
198.818856	6812.591398	8.505293	-0.041779	4.454707
198.985311	6820.607752	8.510298	-0.041815	4.457244
199.055463	6828.578570	8.515302	-0.041834	4.459764
199.082799	6836.611772	8.520307	-0.041845	4.462303
199.354147	6844.621938	8.525312	-0.041901	4.464833
199.396839	6852.669128	8.530317	-0.041914	4.467373
199.466881	6860.641408	8.535322	-0.041933	4.469888
199.753593	6868.730663	8.540326	-0.041992	4.472440
199.654035	6876.715973	8.545331	-0.041978	4.474955
199.853294	6884.746109	8.550336	-0.042021	4.477485
199.811164	6892.715995	8.555341	-0.042019	4.479993
199.954688	6900.756883	8.560346	-0.042051	4.482523
200.064650	6908.731204	8.565351	-0.042077	4.485030
200.022699	6916.739413	8.570355	-0.042075	4.487546
200.418069	6924.802443	8.575360	-0.042154	4.490079
200.343532	6932.831999	8.580365	-0.042145	4.492599
200.556514	6940.811514	8.585370	-0.042190	4.495103
200.598638	6948.855948	8.590375	-0.042204	4.497625
200.776662	6956.837889	8.595379	-0.042242	4.500126
200.843380	6964.884190	8.600384	-0.042260	4.502646
200.991092	6972.851498	8.605389	-0.042293	4.505140
201.244128	6980.899258	8.610394	-0.042346	4.507657
201.528362	6988.940375	8.615399	-0.042404	4.510172
201.385311	6997.016600	8.620403	-0.042383	4.512695
201.644609	7005.064064	8.625408	-0.042437	4.515208
201.661025	7012.990941	8.630413	-0.042446	4.517682
201.838083	7020.956994	8.635418	-0.042484	4.520167
201.722247	7029.011833	8.640423	-0.042468	4.522678
201.974104	7036.962199	8.645427	-0.042520	4.525156
202.058927	7045.000444	8.650432	-0.042542	4.527659
202.189018	7052.994703	8.655437	-0.042571	4.530147
202.295037	7061.069881	8.660442	-0.042597	4.532659
202.507120	7069.096665	8.665447	-0.042642	4.535155
202.746284	7077.080553	8.670451	-0.042692	4.537636
202.787493	7085.072127	8.675456	-0.042705	4.540118
202.708757	7093.088929	8.680461	-0.042696	4.542605
202.955225	7101.119325	8.685466	-0.042747	4.545097
203.219421	7109.189393	8.690471	-0.042802	4.547599
203.315995	7117.148999	8.695475	-0.042825	4.550065
203.527993	7125.207174	8.700480	-0.042870	4.552561
203.497214	7133.234731	8.705485	-0.042870	4.555046
203.753088	7141.235027	8.710490	-0.042923	4.557521
203.922062	7149.212902	8.715495	-0.042960	4.559988
203.735860	7157.214900	8.720499	-0.042931	4.562460
203.986335	7165.208245	8.725504	-0.042983	4.564929
203.981443	7173.264700	8.730509	-0.042987	4.567415
204.150623	7181.266185	8.735514	-0.043024	4.569884
204.225092	7189.321026	8.740519	-0.043044	4.572367
204.452138	7197.324033	8.745523	-0.043092	4.574834
204.612186	7205.367156	8.750528	-0.043127	4.577311
204.736615	7213.317420	8.755533	-0.043156	4.579759
204.698532	7221.425720	8.760538	-0.043154	4.582253
205.083515	7229.379918	8.765543	-0.043231	4.584699
205.199944	7237.437731	8.770547	-0.043258	4.587175
205.340140	7245.471433	8.775552	-0.043290	4.589643
205.136573	7253.524449	8.780557	-0.043258	4.592115
205.308202	7261.477240	8.785562	-0.043295	4.594555
205.634123	7269.554252	8.790567	-0.043361	4.597032
205.615777	7277.480349	8.795571	-0.043363	4.599461
205.600894	7285.547240	8.800576	-0.043366	4.601933
205.778574	7293.492811	8.805581	-0.043405	4.604365
205.927828	7301.573316	8.810586	-0.043438	4.606838
205.984026	7309.571494	8.815591	-0.043454	4.609284
206.202660	7317.612702	8.820595	-0.043500	4.611742
206.136791	7325.643030	8.825600	-0.043493	4.614195
206.323094	7333.655102	8.830605	-0.043533	4.616642
206.494965	7341.606011	8.835610	-0.043571	4.619068
206.549398	7349.659424	8.840615	-0.043587	4.621524
206.647293	7357.622932	8.845619	-0.043610	4.623952
206.972320	7365.686153	8.850624	-0.043676	4.626409
207.162651	7373.684965	8.855629	-0.043717	4.628845
207.120749	7381.731932	8.860634	-0.043715	4.631294
207.320104	7389.749590	8.865639	-0.043758	4.633733
207.381197	7397.771351	8.870643	-0.043774	4.636172
207.578324	7405.759575	8.875648	-0.043817	4.638599
207.588937	7413.765082	8.880653	-0.043824	4.641030
207.722992	7421.742137	8.885658	-0.043854	4.643452
207.754194	7429.793172	8.890663	-0.043866	4.645894
208.100324	7437.815261	8.895667	-0.043936	4.648327
208.226250	7445.831833	8.900672	-0.043965	4.650756
208.155486	7453.898482	8.905677	-0.043957	4.653200
208.144493	7461.887018	8.910682	-0.043960	4.655619
208.331121	7469.895836	8.915687	-0.044001	4.658042
208.444582	7477.850830	8.920691	-0.044027	4.660448
208.547124	7485.909122	8.925696	-0.044052	4.662883
208.638598	7493.940625	8.930701	-0.044074	4.665310
208.956755	7501.930730	8.935706	-0.044139	4.667722
208.890639	7509.942101	8.940711	-0.044132	4.670140
208.950604	7518.031665	8.945715	-0.044149	4.672580
209.230535	7526.104754	8.950720	-0.044207	4.675014
209.188534	7534.007552	8.955725	-0.044204	4.677395
209.402681	7542.005857	8.960730	-0.044250	4.679804
209.455894	7550.063556	8.965735	-0.044265	4.682230
209.606230	7557.961994	8.970739	-0.044298	4.684606
209.610042	7566.031919	8.975744	-0.044305	4.687032
209.718144	7574.035988	8.980749	-0.044330	4.689438
209.999617	7582.087873	8.985754	-0.044388	4.691856
210.081448	7590.112636	8.990759	-0.044409	4.694265
210.020738	7598.136491	8.995763	-0.044403	4.696673
210.144415	7606.129219	9.000768	-0.044432	4.699071
210.215104	7614.141351	9.005773	-0.044450	4.701472
210.332206	7622.096447	9.010778	-0.044478	4.703856
210.555848	7630.181523	9.015783	-0.044525	4.706276
210.712339	7638.162904	9.020787	-0.044559	4.708665
210.622027	7646.193520	9.025792	-0.044548	4.711068
210.694822	7654.232603	9.030797	-0.044567	4.713471
210.940231	7662.251070	9.035802	-0.044618	4.715867
211.281682	7670.232680	9.040807	-0.044687	4.718251
211.198605	7678.254684	9.045811	-0.044677	4.720646
211.408417	7686.293695	9.050816	-0.044722	4.723044
211.523342	7694.279516	9.055821	-0.044749	4.725426
211.712852	7702.363315	9.060826	-0.044790	4.727835
211.837073	7710.342770	9.065831	-0.044818	4.730212
211.869318	7718.343269	9.070835	-0.044830	4.732594
211.951242	7726.423831	9.075840	-0.044851	4.734999
212.017177	7734.431757	9.080845	-0.044868	4.737381
212.240977	7742.404346	9.085850	-0.044916	4.739751
212.170909	7750.489445	9.090855	-0.044908	4.742154
212.300397	7758.386181	9.095859	-0.044938	4.744499
212.768989	7766.472392	9.100864	-0.045030	4.746899
212.822981	7774.486909	9.105869	-0.045046	4.749277
212.854156	7782.501012	9.110874	-0.045057	4.751654
212.992228	7790.580374	9.115879	-0.045088	4.754048
213.225577	7798.549005	9.120883	-0.045137	4.756408
213.309852	7806.571658	9.125888	-0.045159	4.758784
213.423620	7814.543842	9.130893	-0.045185	4.761143
213.623995	7822.487278	9.135898	-0.045228	4.763492
213.862452	7830.546065	9.140903	-0.045278	4.765875
213.850267	7838.538303	9.145907	-0.045281	4.768237
213.905424	7846.631543	9.150912	-0.045297	4.770627
214.018784	7854.607971	9.155917	-0.045323	4.772982
213.873117	7862.637990	9.160922	-0.045302	4.775352
214.118955	7870.638917	9.165927	-0.045353	4.777711
214.149202	7878.633646	9.170931	-0.045364	4.780068
214.376267	7886.676303	9.175936	-0.045412	4.782437
214.417604	7894.653725	9.180941	-0.045425	4.784786
214.675223	7902.709143	9.185946	-0.045479	4.787156
214.830490	7910.688691	9.190951	-0.045513	4.789503
214.910936	7918.734876	9.195955	-0.045534	4.791869
215.302105	7926.740662	9.200960	-0.045612	4.794221
215.311896	7934.801329	9.205965	-0.045619	4.796589
215.242769	7942.692547	9.210970	-0.045612	4.798906
215.471627	7950.851622	9.215975	-0.045660	4.801300
215.354966	7958.775446	9.220979	-0.045644	4.803625
215.592487	7966.794763	9.225984	-0.045693	4.805975
215.578683	7974.822733	9.230989	-0.045696	4.808328
215.584554	7982.835757	9.235994	-0.045703	4.810675
215.895608	7990.370118	9.240999	-0.045766	4.812879
215.801007	7995.022815	9.246003	-0.045752	4.814242

216.030748	7997.629944	9.251008	-0.045796	4.815003
216.133510	7998.970841	9.256013	-0.045817	4.815395
216.166792	7999.421746	9.261018	-0.045823	4.815527
216.125540	8000.478718	9.266023	-0.045817	4.815836
216.406895	8000.442724	9.271027	-0.045869	4.815824
216.583485	8000.480815	9.276032	-0.045903	4.815835
216.590181	8000.466005	9.281037	-0.045904	4.815830
216.584557	8000.460601	9.286042	-0.045903	4.815829
216.762169	8000.483768	9.291047	-0.045937	4.815835
216.650403	8000.467047	9.296051	-0.045916	4.815830
216.673914	8000.468517	9.301056	-0.045921	4.815831
216.656996	8000.501353	9.306061	-0.045918	4.815840
216.661937	8000.471572	9.311066	-0.045919	4.815832
216.820676	8000.505107	9.316071	-0.045949	4.815841
216.691028	8000.469954	9.321075	-0.045925	4.815831
216.926180	8000.490848	9.326080	-0.045969	4.815836
216.679732	8000.458078	9.331085	-0.045923	4.815828
216.879629	8000.394089	9.336090	-0.045961	4.815808
216.984220	8000.486518	9.341095	-0.045981	4.815834
216.934731	8000.453725	9.346099	-0.045972	4.815825
217.059829	8000.472843	9.351104	-0.045995	4.815830
217.155741	8000.485087	9.356109	-0.046013	4.815833
217.433773	8000.470386	9.361114	-0.046065	4.815828
217.297265	8000.448995	9.366119	-0.046040	4.815822
217.126194	8000.482546	9.371123	-0.046009	4.815833
217.234556	8000.507798	9.376128	-0.046029	4.815839
217.226324	8000.461795	9.381133	-0.046028	4.815826
217.235718	8000.499325	9.386138	-0.046030	4.815837
217.219440	8000.521499	9.391143	-0.046027	4.815843
217.084912	8000.406220	9.396147	-0.046002	4.815810
217.036778	8000.457763	9.401152	-0.045994	4.815826
217.086123	8000.518350	9.406157	-0.046003	4.815843
217.342266	8000.507565	9.411162	-0.046051	4.815839
217.291557	8000.486492	9.416167	-0.046042	4.815833
217.522674	8000.469967	9.421171	-0.046085	4.815827
217.550593	8000.424548	9.426176	-0.046091	4.815813
217.563573	8000.530442	9.431181	-0.046093	4.815844
217.469905	8000.507608	9.436186	-0.046076	4.815838
217.719531	8000.412402	9.441191	-0.046123	4.815809
217.826951	8000.467524	9.446195	-0.046143	4.815825
217.587719	8000.498907	9.451200	-0.046099	4.815835
217.493827	8000.495280	9.456205	-0.046082	4.815834
217.724262	8000.478744	9.461210	-0.046125	4.815828
217.542790	8000.437417	9.466215	-0.046091	4.815817
217.403768	8000.505637	9.471219	-0.046066	4.815838
217.497221	8000.539188	9.476224	-0.046084	4.815847
217.416449	8000.432246	9.481229	-0.046069	4.815816
217.341411	8000.483355	9.486234	-0.046055	4.815832
217.510581	8000.493580	9.491239	-0.046087	4.815834
217.672777	8000.482347	9.496243	-0.046117	4.815830
217.664418	8000.472629	9.501248	-0.046116	4.815827
217.681039	8000.473988	9.506253	-0.046119	4.815827
217.818378	8000.446344	9.511258	-0.046145	4.815818
217.761387	8000.558581	9.516263	-0.046135	4.815852
217.704394	8000.491512	9.521267	-0.046124	4.815832
217.902630	8000.415756	9.526272	-0.046162	4.815809
217.877793	8000.525310	9.531277	-0.046157	4.815841
217.815992	8000.462432	9.536282	-0.046146	4.815823
217.956120	8000.491400	9.541287	-0.046172	4.815831
217.897754	8000.517164	9.546291	-0.046162	4.815839
217.882613	8000.476386	9.551296	-0.046159	4.815827
217.962388	8000.540667	9.556301	-0.046174	4.815845
217.949844	8000.498864	9.561306	-0.046172	4.815833
217.769958	8000.430878	9.566311	-0.046139	4.815814
217.882898	8000.495695	9.571315	-0.046160	4.815833
217.983008	8000.520815	9.576320	-0.046179	4.815839
218.028112	8000.453260	9.581325	-0.046188	4.815819
218.073973	8000.483908	9.586330	-0.046197	4.815828
217.931459	8000.464554	9.591335	-0.046171	4.815823
217.701141	8000.449119	9.596339	-0.046128	4.815820
218.000965	8000.510549	9.601344	-0.046184	4.815836
217.813834	8000.461658	9.606349	-0.046149	4.815823
217.902882	8000.488734	9.611354	-0.046166	4.815830
218.045121	8000.513467	9.616359	-0.046193	4.815837
217.983151	8000.431375	9.621363	-0.046182	4.815813
218.036422	8000.522979	9.626368	-0.046192	4.815840
218.098012	8000.528266	9.631373	-0.046204	4.815841
217.903923	8000.416292	9.636378	-0.046168	4.815809
217.738032	8000.511829	9.641383	-0.046137	4.815838
217.888919	8000.520692	9.646387	-0.046166	4.815840
217.992565	8000.456216	9.651392	-0.046185	4.815820
217.868502	8000.517207	9.656397	-0.046162	4.815839
218.023951	8000.502663	9.661402	-0.046192	4.815834
218.181406	8000.431584	9.666407	-0.046221	4.815812
217.854007	8000.510639	9.671411	-0.046160	4.815837
217.974004	8000.505129	9.676416	-0.046183	4.815835
218.073138	8000.495012	9.681421	-0.046202	4.815831
218.178768	8000.447645	9.686426	-0.046222	4.815817
218.277827	8000.526114	9.691431	-0.046240	4.815839
218.289481	8000.442008	9.696435	-0.046243	4.815815
218.250614	8000.473423	9.701440	-0.046236	4.815824
218.213090	8000.540081	9.706445	-0.046229	4.815844
218.277793	8000.494188	9.711450	-0.046242	4.815830
218.279430	8000.465420	9.716455	-0.046242	4.815822
218.035048	8000.515931	9.721459	-0.046197	4.815838
218.134777	8000.560257	9.726464	-0.046216	4.815850
218.185621	8000.446899	9.731469	-0.046225	4.815817
218.129764	8000.519665	9.736474	-0.046215	4.815838
218.049205	8000.486369	9.741479	-0.046201	4.815829
218.285662	8000.433642	9.746483	-0.046245	4.815812
218.218144	8000.559585	9.751488	-0.046233	4.815849
218.360034	8000.459438	9.756493	-0.046259	4.815819
218.444007	8000.514183	9.761498	-0.046275	4.815835
218.476978	8000.462440	9.766503	-0.046282	4.815820
218.230879	8000.532135	9.771507	-0.046236	4.815841
218.230849	8000.455311	9.776512	-0.046236	4.815819
218.389967	8000.478183	9.781517	-0.046266	4.815825
218.309289	8000.508923	9.786522	-0.046251	4.815834
218.214967	8000.568260	9.791527	-0.046234	4.815852
218.257001	8000.449423	9.796531	-0.046242	4.815817
218.505334	8000.469466	9.801536	-0.046289	4.815822
218.427770	8000.486381	9.806541	-0.046275	4.815827
218.406660	8000.519151	9.811546	-0.046271	4.815837
218.444017	8000.434392	9.816551	-0.046278	4.815812
218.318603	8000.544459	9.821555	-0.046255	4.815844
218.334797	8000.443349	9.826560	-0.046258	4.815815
218.542367	8000.507561	9.831565	-0.046297	4.815833
218.480630	8000.531135	9.836570	-0.046286	4.815840
218.424618	8000.490764	9.841575	-0.046276	4.815828
218.663478	8000.485038	9.846579	-0.046321	4.815825
218.524494	8000.557530	9.851584	-0.046295	4.815847
218.487291	8000.487577	9.856589	-0.046288	4.815827
218.499263	8000.432293	9.861594	-0.046291	4.815811
218.702713	8000.506045	9.866599	-0.046329	4.815831
218.439694	8000.447388	9.871603	-0.046280	4.815815
218.514079	8000.457151	9.876608	-0.046294	4.815818
218.489515	8000.473855	9.881613	-0.046290	4.815823
218.487836	8000.538957	9.886618	-0.046290	4.815842
218.386095	8000.487174	9.891623	-0.046271	4.815827
218.122466	8000.467999	9.896627	-0.046223	4.815823
218.339391	8000.374399	9.901632	-0.046263	4.815794
218.297071	8000.576529	9.906637	-0.046256	4.815854
218.261316	8000.459638	9.911642	-0.046249	4.815820
218.644154	8000.516006	9.916647	-0.046321	4.815834
218.529683	8000.546201	9.921651	-0.046300	4.815844
218.557597	8000.367366	9.926656	-0.046305	4.815791
218.518311	8000.518314	9.931661	-0.046298	4.815836
218.467067	8000.440663	9.936666	-0.046289	4.815813
218.588244	8000.479999	9.941671	-0.046312	4.815824
218.508247	8000.473394	9.946675	-0.046297	4.815823
218.709009	8000.476660	9.951680	-0.046335	4.815823
218.562023	8000.425213	9.956685	-0.046308	4.815808
218.584206	8000.551538	9.961690	-0.046312	4.815845
218.593326	8000.442842	9.966695	-0.046314	4.815813
218.459697	8000.452449	9.971699	-0.046289	4.815817
218.332614	8000.448286	9.976704	-0.046266	4.815816
218.253198	8000.560162	9.981709	-0.046252	4.815849
218.379429	8000.427742	9.986714	-0.046275	4.815810
218.549534	8000.499888	9.991719	-0.046307	4.815830
218.444048	8000.515285	9.996723	-0.046288	4.815835
218.513942	8000.550591	10.001728	-0.046301	4.815845
218.664661	8000.472999	10.006733	-0.046329	4.815822
218.448350	8000.422568	10.011738	-0.046289	4.815808
218.642081	8000.496163	10.016743	-0.046326	4.815828
218.556142	8000.540693	10.021747	-0.046310	4.815842
218.512790	8000.386323	10.026752	-0.046302	4.815797
218.505830	8000.485494	10.031757	-0.046301	4.815826
218.574138	8000.525044	10.036762	-0.046314	4.815837
218.552848	8000.534330	10.041767	-0.046311	4.815840
218.543591	8000.511790	10.046771	-0.046309	4.815833
218.653322	8000.407921	10.051776	-0.046330	4.815803
218.606925	8000.502186	10.056781	-0.046321	4.815830
218.485402	8000.436208	10.061786	-0.046299	4.815812
218.571427	8000.556093	10.066791	-0.046315	4.815846
218.656799	8000.450763	10.071795	-0.046332	4.815815
218.488269	8000.551595	10.076800	-0.046300	4.815845
218.549199	8000.483227	10.081805	-0.046312	4.815825
218.550619	8000.538774	10.086810	-0.046313	4.815841
218.694279	8000.456799	10.091815	-0.046340	4.815817
218.513388	8000.519008	10.096819	-0.046306	4.815836
218.642396	8000.438931	10.101824	-0.046330	4.815812
218.582710	8000.490289	10.106829	-0.046320	4.815827
218.677296	8000.461955	10.111834	-0.046338	4.815818
218.741599	8000.470488	10.116839	-0.046350	4.815820
218.673676	8000.487559	10.121843	-0.046337	4.815826
218.696049	8000.492213	10.126848	-0.046342	4.815827
218.675677	8000.568755	10.131853	-0.046338	4.815849
218.658914	8000.422284	10.136858	-0.046335	4.815807
218.524081	8000.536468	10.141863	-0.046311	4.815841
218.362507	8000.521075	10.146867	-0.046281	4.815837
218.486445	8000.460128	10.151872	-0.046304	4.815818
218.642433	8000.478680	10.156877	-0.046333	4.815823
218.749430	8000.519922	10.161882	-0.046354	4.815835
218.675668	8000.468590	10.166887	-0.046340	4.815820
218.622138	8000.542462	10.171891	-0.046331	4.815842
218.607966	8000.456871	10.176896	-0.046328	4.815817
218.753513	8000.546765	10.181901	-0.046356	4.815843
218.838515	8000.442496	10.186906	-0.046372	4.815812
218.942847	8000.489032	10.191911	-0.046391	4.815825
218.574161	8000.507650	10.196915	-0.046323	4.815832
218.636529	8000.477728	10.201920	-0.046335	4.815823
218.717145	8000.533487	10.206925	-0.046350	4.815839
218.705357	8000.410578	10.211930	-0.046348	4.815803
218.720549	8000.490896	10.216935	-0.046351	4.815826
218.684765	8000.524496	10.221939	-0.046345	4.815836
218.666151	8000.472987	10.226944	-0.046342	4.815821
218.591199	8000.484608	10.231949	-0.046328	4.815825
218.530236	8000.503926	10.236954	-0.046317	4.815831
218.668692	8000.531801	10.241959	-0.046343	4.815838
218.590715	8000.419564	10.246963	-0.046329	4.815806
218.883182	8000.517168	10.251968	-0.046383	4.815833
219.003003	8000.502049	10.256973	-0.046406	4.815828
218.890182	8000.472500	10.261978	-0.046385	4.815820
218.969387	8000.504755	10.266983	-0.046400	4.815829
219.025105	8000.518486	10.271987	-0.046411	4.815833
218.811093	8000.455283	10.276992	-0.046371	4.815815
218.735250	8000.541602	10.281997	-0.046358	4.815841
218.889270	8000.508891	10.287002	-0.046386	4.815831
218.993833	8000.459372	10.292007	-0.046406	4.815816
218.734400	8000.491494	10.297011	-0.046358	4.815826
218.776380	8000.530620	10.302016	-0.046366	4.815838
218.951394	8000.487575	10.307021	-0.046399	4.815824
218.929364	8000.528868	10.312026	-0.046395	4.815836
218.953948	8000.463114	10.317031	-0.046400	4.815817
218.833028	8000.486800	10.322035	-0.046378	4.815824
218.814354	8000.429954	10.327040	-0.046375	4.815808
218.846626	8000.473192	10.332045	-0.046381	4.815820
219.039814	8000.537173	10.337050	-0.046417	4.815838
219.009771	8000.472671	10.342055	-0.046412	4.815819
218.783195	8000.525604	10.347059	-0.046370	4.815836
218.786972	8000.461649	10.352064	-0.046371	4.815817
218.830161	8000.559497	10.357069	-0.046379	4.815846
218.818358	8000.425914	10.362074	-0.046377	4.815807
218.739810	8000.476967	10.367079	-0.046363	4.815822
218.966271	8000.540419	10.372083	-0.046405	4.815839
219.004995	8000.521856	10.377088	-0.046413	4.815834
218.883303	8000.429191	10.382093	-0.046390	4.815807
218.944063	8000.514514	10.387098	-0.046402	4.815832
219.178021	8000.539664	10.392103	-0.046446	4.815838
218.889171	8000.458174	10.397107	-0.046392	4.815816
218.787532	8000.504585	10.402112	-0.046374	4.815830
218.843205	8000.471353	10.407117	-0.046384	4.815820
218.889956	8000.516960	10.412122	-0.046393	4.815833
218.703828	8000.473419	10.417127	-0.046359	4.815821
218.873316	8000.542354	10.422131	-0.046391	4.815840
218.887578	8000.439077	10.427136	-0.046394	4.815810
218.681467	8000.513686	10.432141	-0.046356	4.815833
218.861979	8000.494211	10.437146	-0.046389	4.815826
219.065615	8000.492187	10.442151	-0.046428	4.815825
218.805287	8000.502948	10.447155	-0.046379	4.815829
218.860062	8000.441951	10.452160	-0.046390	4.815811
219.063433	8000.545589	10.457165	-0.046428	4.815840
219.080727	8000.519208	10.462170	-0.046432	4.815833
218.957894	8000.408380	10.467175	-0.046409	4.815801
218.944696	8000.493576	10.472179	-0.046407	4.815826
219.007506	8000.464729	10.477184	-0.046419	4.815817
219.102164	8000.573015	10.482189	-0.046437	4.815848
218.597164	8000.450678	10.487194	-0.046343	4.815815
219.036135	8000.465262	10.492199	-0.046425	4.815817
219.023509	8000.529121	10.497203	-0.046423	4.815836
219.147132	8000.341156	10.502208	-0.046446	4.815780
218.988002	8000.405852	10.507213	-0.046417	4.815800
219.150155	8000.549382	10.512218	-0.046447	4.815841
219.011402	8000.413748	10.517223	-0.046422	4.815802
219.067158	8000.558762	10.522227	-0.046432	4.815844
219.018193	8000.458732	10.527232	-0.046423	4.815815
219.225722	8000.549629	10.532237	-0.046462	4.815841
219.172311	8000.529578	10.537242	-0.046453	4.815835
219.136291	8000.466046	10.542247	-0.046446	4.815817
218.933922	8000.519370	10.547251	-0.046409	4.815833
219.019676	8000.514374	10.552256	-0.046425	4.815831
219.116504	8000.466865	10.557261	-0.046443	4.815817
219.187169	8000.528868	10.562266	-0.046457	4.815835
219.127539	8000.534332	10.567271	-0.046446	4.815837
219.239202	8000.529755	10.572275	-0.046467	4.815835
219.378439	8000.454112	10.577280	-0.046493	4.815812
219.150318	8000.536905	10.582285	-0.046451	4.815837
218.976881	8000.512780	10.587290	-0.046419	4.815831
219.134913	8000.568723	10.592295	-0.046449	4.815847
219.248925	8000.424363	10.597299	-0.046470	4.815804
219.208572	8000.528334	10.602304	-0.046463	4.815834
219.329431	8000.523905	10.607309	-0.046486	4.815833
219.234150	8000.527726	10.612314	-0.046468	4.815834
219.103514	8000.445589	10.617319	-0.046444	4.815811
218.974896	8000.527855	10.622323	-0.046421	4.815835
219.154245	8000.533977	10.627328	-0.046454	4.815836
219.051816	8000.521673	10.632333	-0.046435	4.815833
218.980625	8000.529085	10.637338	-0.046422	4.815836
219.422982	8000.429520	10.642343	-0.046505	4.815804
219.301546	8000.510834	10.647347	-0.046483	4.815829
219.159500	8000.537381	10.652352	-0.046457	4.815837
218.940596	8000.479435	10.657357	-0.046416	4.815821
219.032376	8000.549250	10.662362	-0.046433	4.815841
219.248355	8000.471645	10.667367	-0.046474	4.815818
219.233143	8000.451143	10.672371	-0.046471	4.815812
219.328591	8000.528489	10.677376	-0.046489	4.815834
219.226787	8000.584505	10.682381	-0.046471	4.815851
219.242603	8000.419346	10.687386	-0.046474	4.815802
219.287401	8000.588733	10.692391	-0.046483	4.815852
219.152312	8000.476638	10.697395	-0.046458	4.815819
219.277489	8000.540589	10.702400	-0.046481	4.815838
219.374658	8000.493085	10.707405	-0.046500	4.815823
219.150818	8000.505502	10.712410	-0.046458	4.815828
219.254259	8000.492254	10.717415	-0.046478	4.815823
219.106906	8000.508042	10.722419	-0.046450	4.815829
219.082335	8000.541823	10.727424	-0.046446	4.815839
219.297019	8000.489813	10.732429	-0.046486	4.815823
219.208793	8000.543913	10.737434	-0.046470	4.815839
219.366682	8000.461099	10.742439	-0.046500	4.815814
219.295042	8000.566700	10.747443	-0.046487	4.815845
219.186509	8000.472111	10.752448	-0.046467	4.815818
219.289921	8000.549587	10.757453	-0.046486	4.815840
219.676972	8000.472610	10.762458	-0.046559	4.815816
219.513950	8000.407027	10.767463	-0.046529	4.815797
219.335966	8000.529054	10.772467	-0.046496	4.815834
219.320455	8000.541635	10.777472	-0.046493	4.815838
219.492607	8000.515621	10.782477	-0.046526	4.815829
219.206680	8000.429908	10.787482	-0.046473	4.815805
219.303927	8000.494475	10.792487	-0.046491	4.815824
219.206376	8000.585782	10.797491	-0.046473	4.815851
219.332764	8000.468304	10.802496	-0.046497	4.815816
219.413066	8000.464288	10.807501	-0.046512	4.815814
219.258443	8000.551471	10.812506	-0.046484	4.815841
219.298179	8000.408045	10.817511	-0.046491	4.815798
219.402292	8000.577323	10.822515	-0.046511	4.815848
219.395623	8000.451292	10.827520	-0.046510	4.815811
219.384595	8000.507707	10.832525	-0.046508	4.815827
219.308517	8000.511838	10.837530	-0.046494	4.815829
219.406951	8000.566819	10.842535	-0.046513	4.815844
219.520529	8000.456606	10.847539	-0.046534	4.815812
219.340008	8000.555111	10.852544	-0.046501	4.815841
219.234837	8000.548098	10.857549	-0.046482	4.815840
219.219385	8000.461417	10.862554	-0.046479	4.815814
219.367768	8000.489454	10.867559	-0.046507	4.815822
219.084986	8000.530805	10.872563	-0.046455	4.815835
219.244611	8000.408528	10.877568	-0.046484	4.815799
219.315988	8000.491890	10.882573	-0.046498	4.815823
219.190880	8000.544327	10.887578	-0.046475	4.815839
219.299560	8000.434035	10.892583	-0.046496	4.815806
219.477491	8000.598102	10.897587	-0.046529	4.815853
219.461780	8000.435635	10.902592	-0.046526	4.815806
219.358854	8000.453208	10.907597	-0.046507	4.815811
219.388338	8000.514546	10.912602	-0.046513	4.815829
219.688513	8000.505544	10.917607	-0.046569	4.815825
219.488229	8000.562103	10.922611	-0.046532	4.815843
219.450693	8000.482536	10.927616	-0.046526	4.815819
219.382354	8000.580719	10.932621	-0.046513	4.815848
219.346809	8000.456356	10.937626	-0.046507	4.815812
219.273463	8000.473339	10.942631	-0.046493	4.815818
219.439268	8000.553958	10.947635	-0.046525	4.815840
219.404703	8000.366638	10.952640	-0.046518	4.815786
219.447799	8000.558412	10.957645	-0.046527	4.815842
219.434173	8000.541138	10.962650	-0.046524	4.815837
219.510339	8000.483687	10.967655	-0.046539	4.815819
219.277405	8000.489554	10.972659	-0.046496	4.815822
219.361195	8000.536827	10.977664	-0.046512	4.815836
219.604198	8000.477803	10.982669	-0.046557	4.815817
219.455588	8000.486099	10.987674	-0.046530	4.815820
219.372422	8000.591513	10.992679	-0.046515	4.815852
219.533402	8000.508750	10.997683	-0.046545	4.815827
219.524661	8000.488352	11.002688	-0.046543	4.815821
219.370680	8000.444262	11.007693	-0.046515	4.815808
219.214414	8000.514340	11.012698	-0.046486	4.815830
219.575313	8000.454018	11.017703	-0.046554	4.815810
219.363135	8000.532800	11.022707	-0.046514	4.815834
219.234068	8000.504054	11.027712	-0.046491	4.815827
219.461322	8000.490672	11.032717	-0.046533	4.815822
219.506996	8000.522386	11.037722	-0.046542	4.815831
219.474468	8000.501604	11.042727	-0.046536	4.815825
219.391231	8000.619826	11.047731	-0.046521	4.815860
219.454563	8000.434087	11.052736	-0.046533	4.815805
219.506498	8000.406131	11.057741	-0.046543	4.815797
219.343532	8000.518795	11.062746	-0.046513	4.815830
219.620167	8000.386667	11.067751	-0.046565	4.815790
219.431039	8000.489303	11.072755	-0.046530	4.815821
219.479384	8000.461289	11.077760	-0.046539	4.815813
219.736100	8000.533771	11.082765	-0.046587	4.815833
219.575817	8000.553619	11.087770	-0.046558	4.815839
219.494274	8000.382616	11.092775	-0.046543	4.815790
219.540300	8000.493320	11.097779	-0.046551	4.815822
219.675442	8000.434688	11.102784	-0.046577	4.815804
219.600023	8000.497534	11.107789	-0.046563	4.815823
219.443808	8000.418184	11.112794	-0.046534	4.815800
219.528997	8000.320321	11.117799	-0.046550	4.815771
219.371803	8000.535543	11.122803	-0.046521	4.815835
219.481171	8000.415656	11.127808	-0.046542	4.815799
219.650243	8000.528348	11.132813	-0.046574	4.815832
219.510417	8000.467408	11.137818	-0.046548	4.815814
219.575011	8000.444994	11.142823	-0.046560	4.815808
219.315697	8000.457905	11.147827	-0.046512	4.815813
219.465447	8000.432597	11.152832	-0.046540	4.815804
219.261790	8000.494438	11.157837	-0.046503	4.815823
219.257218	8000.510398	11.162842	-0.046502	4.815828
219.543209	8000.362411	11.167847	-0.046556	4.815784
219.525749	8000.520120	11.172851	-0.046553	4.815830
219.349714	8000.549320	11.177856	-0.046520	4.815839
219.580453	8000.491165	11.182861	-0.046564	4.815821
219.733331	8000.447762	11.187866	-0.046592	4.815808
219.567668	8000.552912	11.192871	-0.046562	4.815839
219.308462	8000.534872	11.197875	-0.046514	4.815835
219.593840	8000.457320	11.202880	-0.046567	4.815811
219.552970	8000.529263	11.207885	-0.046560	4.815832
219.426372	8000.453594	11.212890	-0.046536	4.815811
219.552841	8000.507961	11.217895	-0.046560	4.815826
219.596729	8000.533242	11.222899	-0.046569	4.815833
219.604015	8000.349799	11.227904	-0.046570	4.815779
219.770454	8000.504076	11.232909	-0.046602	4.815824
219.763258	8000.550947	11.237914	-0.046601	4.815838
219.736688	8000.519587	11.242919	-0.046596	4.815828
219.610068	8000.427907	11.247923	-0.046573	4.815802
219.639125	8000.536203	11.252928	-0.046578	4.815834
219.711362	8000.508575	11.257933	-0.046592	4.815825
219.442602	8000.458360	11.262938	-0.046542	4.815812
219.805702	8000.383131	11.267943	-0.046610	4.815788
219.884275	8000.543460	11.272947	-0.046625	4.815835
219.751674	8000.394046	11.277952	-0.046600	4.815792
219.632558	8000.329171	11.282957	-0.046579	4.815773
219.739432	8000.450465	11.287962	-0.046599	4.815808
219.703299	8000.351708	11.292967	-0.046592	4.815779
219.425322	8000.494535	11.297971	-0.046541	4.815823
219.569563	8000.486215	11.302976	-0.046568	4.815819
219.827498	8000.434904	11.307981	-0.046616	4.815803
219.618007	8000.501988	11.312986	-0.046578	4.815824
219.706121	8000.309177	11.317991	-0.046594	4.815767
219.611814	8000.401603	11.322995	-0.046577	4.815794
219.745656	8000.497716	11.328000	-0.046602	4.815822
219.628556	8000.425402	11.333005	-0.046581	4.815801
219.813177	8000.377176	11.338010	-0.046615	4.815786
219.756276	8000.478746	11.343015	-0.046605	4.815816
219.743077	8000.496701	11.348019	-0.046603	4.815822
219.578764	8000.500474	11.353024	-0.046572	4.815823
219.640541	8000.579413	11.358029	-0.046584	4.815846
219.519775	8000.536925	11.363034	-0.046562	4.815834
219.671847	8000.394245	11.368039	-0.046590	4.815792
219.546445	8000.590771	11.373043	-0.046568	4.815850
219.619661	8000.410527	11.378048	-0.046581	4.815797
219.721800	8000.410066	11.383053	-0.046601	4.815796
219.580852	8000.512413	11.388058	-0.046575	4.815827
219.835616	8000.431164	11.393063	-0.046622	4.815802
219.657813	8000.591620	11.398067	-0.046590	4.815850
219.755153	8000.450190	11.403072	-0.046608	4.815808
219.967393	8000.347975	11.408077	-0.046648	4.815777
219.607083	8000.525762	11.413082	-0.046581	4.815831
219.683021	8000.458702	11.418087	-0.046595	4.815811
219.689657	8000.431081	11.423091	-0.046597	4.815803
219.569044	8000.464378	11.428096	-0.046575	4.815813
219.658900	8000.462652	11.433101	-0.046592	4.815812
219.634041	8000.541258	11.438106	-0.046587	4.815835
219.760399	8000.387489	11.443111	-0.046611	4.815789
219.700818	8000.498622	11.448115	-0.046600	4.815822
219.776404	8000.479587	11.453120	-0.046615	4.815816
219.861081	8000.430813	11.458125	-0.046631	4.815802
219.610237	8000.561270	11.463130	-0.046584	4.815841
219.750521	8000.463229	11.468135	-0.046611	4.815812
219.938208	8000.482295	11.473139	-0.046646	4.815816
219.648614	8000.508593	11.478144	-0.046592	4.815825
219.643831	8000.434891	11.483149	-0.046591	4.815804
219.719542	8000.567423	11.488154	-0.046606	4.815842
219.849497	8000.471349	11.493159	-0.046630	4.815813
219.627952	8000.554249	11.498163	-0.046589	4.815839
219.762986	8000.466796	11.503168	-0.046615	4.815813
219.989545	8000.487559	11.508173	-0.046657	4.815818
219.839783	8000.570551	11.513178	-0.046630	4.815843
219.768509	8000.474427	11.518183	-0.046617	4.815815
219.875573	8000.488989	11.523187	-0.046637	4.815818
219.903469	8000.397671	11.528192	-0.046642	4.815792
219.848221	8000.416014	11.533197	-0.046632	4.815797
219.755684	8000.444428	11.538202	-0.046615	4.815806
219.802090	8000.408911	11.543207	-0.046624	4.815795
219.573925	8000.489569	11.548211	-0.046582	4.815820
219.682703	8000.560729	11.553216	-0.046603	4.815840
219.949369	8000.499952	11.558221	-0.046652	4.815821
219.716101	8000.451377	11.563226	-0.046609	4.815808
219.469706	8000.455958	11.568231	-0.046564	4.815811
219.858742	8000.500693	11.573235	-0.046636	4.815822
219.965049	8000.469346	11.578240	-0.046656	4.815812
219.651093	8000.525136	11.583245	-0.046598	4.815830
219.777624	8000.464229	11.588250	-0.046622	4.815812
220.122409	8000.419658	11.593255	-0.046687	4.815797
219.972625	8000.576299	11.598259	-0.046659	4.815843
219.636785	8000.491910	11.603264	-0.046597	4.815820
219.721499	8000.499706	11.608269	-0.046613	4.815822
219.693421	8000.487535	11.613274	-0.046608	4.815819
219.501088	8000.383053	11.618279	-0.046572	4.815789
219.513772	8000.431312	11.623283	-0.046575	4.815803
219.691691	8000.553754	11.628288	-0.046608	4.815838
219.676464	8000.417977	11.633293	-0.046606	4.815798
219.717658	8000.509391	11.638298	-0.046614	4.815825
219.927274	8000.363372	11.643303	-0.046653	4.815781
219.836208	8000.502815	11.648307	-0.046636	4.815823
219.950008	8000.479061	11.653312	-0.046658	4.815815
219.992867	8000.476575	11.658317	-0.046666	4.815814
219.702783	8000.553030	11.663322	-0.046612	4.815838
219.696784	8000.422739	11.668327	-0.046611	4.815800
219.715011	8000.496704	11.673331	-0.046615	4.815821
219.840135	8000.463527	11.678336	-0.046639	4.815811
219.785045	8000.489344	11.683341	-0.046629	4.815819
219.709723	8000.569270	11.688346	-0.046615	4.815843
219.956239	8000.389691	11.693351	-0.046661	4.815789
219.816738	8000.512341	11.698355	-0.046635	4.815825
219.696622	8000.321502	11.703360	-0.046613	4.815770
219.839501	8000.440175	11.708365	-0.046640	4.815804
219.885995	8000.574371	11.713370	-0.046649	4.815843
219.923321	8000.281473	11.718375	-0.046656	4.815757
219.852673	8000.395630	11.723379	-0.046643	4.815791
219.771179	8000.367652	11.728384	-0.046628	4.815783
219.946130	8000.365166	11.733389	-0.046661	4.815782
219.722493	8000.484322	11.738394	-0.046620	4.815818
219.868280	8000.498442	11.743399	-0.046647	4.815821
219.887562	8000.600177	11.748403	-0.046651	4.815851
219.735867	8000.389614	11.753408	-0.046623	4.815790
219.767315	8000.383741	11.758413	-0.046629	4.815788
219.752808	8000.536162	11.763418	-0.046627	4.815833
219.811516	8000.481632	11.768423	-0.046638	4.815816
219.668923	8000.439859	11.773427	-0.046612	4.815805
219.929632	8000.456903	11.778432	-0.046661	4.815808
219.902411	8000.514124	11.783437	-0.046656	4.815825
219.818435	8000.439143	11.788442	-0.046640	4.815804
220.153969	8000.477677	11.793447	-0.046703	4.815813
220.034094	8000.487504	11.798451	-0.046681	4.815817
219.912519	8000.458879	11.803456	-0.046659	4.815809
219.854100	8000.409927	11.808461	-0.046648	4.815795
219.876500	8000.504240	11.813466	-0.046653	4.815823
219.897676	8000.491797	11.818471	-0.046657	4.815819
219.918514	8000.508168	11.823475	-0.046661	4.815823
219.997454	8000.466773	11.828480	-0.046676	4.815811
220.020953	8000.493860	11.833485	-0.046681	4.815819
219.963044	8000.486543	11.838490	-0.046670	4.815817
219.960889	8000.403278	11.843495	-0.046670	4.815793
219.954851	8000.591060	11.848499	-0.046669	4.815848
220.040515	8000.484664	11.853504	-0.046685	4.815816
220.070541	8000.510789	11.858509	-0.046691	4.815823
220.065838	8000.519276	11.863514	-0.046691	4.815826
220.005185	8000.412650	11.868519	-0.046680	4.815795
219.927569	8000.414621	11.873523	-0.046665	4.815796
219.869110	8000.459596	11.878528	-0.046655	4.815809
220.031666	8000.435562	11.883533	-0.046685	4.815802
219.824817	8000.488813	11.888538	-0.046647	4.815818
220.152543	8000.400205	11.893543	-0.046708	4.815791
220.052641	8000.459454	11.898547	-0.046690	4.815808
219.865109	8000.352913	11.903552	-0.046655	4.815778
219.852316	8000.457331	11.908557	-0.046653	4.815809
219.896556	8000.442059	11.913562	-0.046662	4.815804
219.955843	8000.356584	11.918567	-0.046673	4.815779
219.919386	8000.388039	11.923571	-0.046667	4.815788
219.923586	8000.464980	11.928576	-0.046668	4.815811
219.975217	8000.359102	11.933581	-0.046677	4.815779
219.752797	8000.557263	11.938586	-0.046636	4.815838
219.694985	8000.514725	11.943591	-0.046626	4.815826
219.805109	8000.410859	11.948595	-0.046647	4.815795
219.874622	8000.480317	11.953600	-0.046660	4.815815
219.988250	8000.565432	11.958605	-0.046681	4.815840
219.924091	8000.480096	11.963610	-0.046670	4.815815
219.995085	8000.493008	11.968615	-0.046683	4.815818
219.874417	8000.572201	11.973619	-0.046661	4.815842
219.912062	8000.487443	11.978624	-0.046668	4.815817
220.058376	8000.433261	11.983629	-0.046696	4.815801
220.018809	8000.552190	11.988634	-0.046689	4.815836
220.113548	8000.495040	11.993639	-0.046707	4.815818
219.966547	8000.440386	11.998643	-0.046679	4.815803
219.837765	8000.450070	12.003648	-0.046656	4.815807
219.857803	8000.485640	12.008653	-0.046660	4.815817
219.836165	8000.549356	12.013658	-0.046656	4.815836
219.994769	8000.501776	12.018663	-0.046686	4.815821
219.948308	8000.479701	12.023667	-0.046677	4.815815
219.983308	8000.499503	12.028672	-0.046684	4.815820
220.108579	8000.499416	12.033677	-0.046708	4.815820
219.937593	8000.575662	12.038682	-0.046676	4.815843
220.047646	8000.394944	12.043687	-0.046697	4.815789
220.174994	8000.497358	12.048691	-0.046721	4.815819
220.128219	8000.520108	12.053696	-0.046713	4.815826
220.135338	8000.511707	12.058701	-0.046714	4.815823
219.965902	8000.549552	12.063706	-0.046683	4.815835
220.130908	8000.431630	12.068711	-0.046714	4.815800
220.043158	8000.492142	12.073715	-0.046698	4.815818
220.251700	8000.473122	12.078720	-0.046737	4.815811
220.308732	8000.523166	12.083725	-0.046748	4.815826
220.171754	8000.576479	12.088730	-0.046723	4.815842
220.255307	8000.444431	12.093735	-0.046738	4.815803
220.403459	8000.508757	12.098739	-0.046766	4.815821
220.336736	8000.399897	12.103744	-0.046754	4.815789
220.100431	8000.508175	12.108749	-0.046710	4.815822
220.077547	8000.561198	12.113754	-0.046706	4.815838
220.254803	8000.484033	12.118759	-0.046740	4.815814
220.163643	8000.493257	12.123763	-0.046723	4.815818
220.233765	8000.455988	12.128768	-0.046736	4.815806
220.338962	8000.584730	12.133773	-0.046756	4.815843
220.275562	8000.454576	12.138778	-0.046745	4.815806
220.281401	8000.489917	12.143783	-0.046746	4.815816
220.114345	8000.506453	12.148787	-0.046715	4.815822
220.224339	8000.387641	12.153792	-0.046736	4.815786
220.162402	8000.266052	12.158797	-0.046724	4.815751
220.173137	8000.384726	12.163802	-0.046727	4.815786
220.302045	8000.378294	12.168807	-0.046751	4.815783
220.189490	8000.504583	12.173811	-0.046730	4.815821
219.904806	8000.542700	12.178816	-0.046678	4.815833
220.048216	8000.487403	12.183821	-0.046705	4.815816
219.978915	8000.553551	12.188826	-0.046692	4.815836
219.950627	8000.496547	12.193831	-0.046687	4.815819
220.002910	8000.563592	12.198835	-0.046697	4.815839
219.958585	8000.447623	12.203840	-0.046689	4.815805
219.917806	8000.576139	12.208845	-0.046682	4.815843
219.952551	8000.459314	12.213850	-0.046688	4.815808
220.146805	8000.510508	12.218855	-0.046725	4.815823
220.305069	8000.530168	12.223859	-0.046755	4.815828
220.151878	8000.544793	12.228864	-0.046726	4.815833
220.146673	8000.427322	12.233869	-0.046726	4.815798
220.176984	8000.566594	12.238874	-0.046732	4.815839
220.173841	8000.458761	12.243879	-0.046731	4.815807
220.135172	8000.568099	12.248883	-0.046724	4.815839
220.192723	8000.439901	12.253888	-0.046735	4.815802
220.090576	8000.594110	12.258893	-0.046717	4.815847
219.991414	8000.539162	12.263898	-0.046698	4.815832
219.914074	8000.469623	12.268903	-0.046684	4.815812
219.972689	8000.464190	12.273907	-0.046695	4.815810
219.904971	8000.497275	12.278912	-0.046683	4.815820
220.172817	8000.571007	12.283917	-0.046733	4.815840
220.235461	8000.506933	12.288922	-0.046745	4.815821
220.299899	8000.462101	12.293927	-0.046757	4.815808
220.121046	8000.480581	12.298931	-0.046724	4.815814
220.206566	8000.557770	12.303936	-0.046741	4.815836
220.328912	8000.397530	12.308941	-0.046764	4.815789
219.993515	8000.463647	12.313946	-0.046701	4.815809
220.242925	8000.348156	12.318951	-0.046748	4.815774
220.220229	8000.497244	12.323955	-0.046744	4.815818
220.115599	8000.417659	12.328960	-0.046725	4.815795
220.205077	8000.404185	12.333965	-0.046742	4.815791
220.315169	8000.511658	12.338970	-0.046763	4.815822
220.194327	8000.423271	12.343975	-0.046740	4.815797
220.031253	8000.522059	12.348979	-0.046710	4.815826
220.245926	8000.458308	12.353984	-0.046751	4.815807
220.315793	8000.366599	12.358989	-0.046764	4.815779
220.158053	8000.506033	12.363994	-0.046735	4.815821
220.090473	8000.454798	12.368999	-0.046722	4.815806
220.114998	8000.525665	12.374003	-0.046727	4.815827
220.036985	8000.461452	12.379008	-0.046713	4.815808
220.406829	8000.502677	12.384013	-0.046782	4.815819
220.266920	8000.435329	12.389018	-0.046756	4.815800
220.343625	8000.366145	12.394023	-0.046771	4.815779
220.225639	8000.427237	12.399027	-0.046749	4.815798
220.174466	8000.381604	12.404032	-0.046740	4.815784
220.296156	8000.468984	12.409037	-0.046763	4.815809
219.926968	8000.458771	12.414042	-0.046694	4.815808
220.138655	8000.499574	12.419047	-0.046734	4.815819
220.166873	8000.428539	12.424051	-0.046740	4.815798
220.035823	8000.449927	12.429056	-0.046716	4.815805
220.117150	8000.482218	12.434061	-0.046731	4.815814
220.170592	8000.457489	12.439066	-0.046741	4.815807
220.136010	8000.499648	12.444071	-0.046735	4.815819
220.187503	8000.515447	12.449075	-0.046745	4.815823
220.220796	8000.469044	12.454080	-0.046751	4.815810
220.289440	8000.390124	12.459085	-0.046764	4.815786
220.104016	8000.526977	12.464090	-0.046730	4.815827
220.168749	8000.465071	12.469095	-0.046742	4.815809
220.255832	8000.417403	12.474099	-0.046759	4.815794
220.368386	8000.427785	12.479104	-0.046780	4.815797
220.333751	8000.514773	12.484109	-0.046774	4.815823
220.151643	8000.535335	12.489114	-0.046740	4.815829
220.307845	8000.500526	12.494119	-0.046770	4.815818
220.268880	8000.552221	12.499123	-0.046763	4.815834
220.305159	8000.475979	12.504128	-0.046770	4.815811
220.344040	8000.509720	12.509133	-0.046777	4.815821
220.037179	8000.529333	12.514138	-0.046720	4.815828
220.049922	8000.418556	12.519143	-0.046723	4.815796
220.259880	8000.489217	12.524147	-0.046762	4.815815
220.079269	8000.471378	12.529152	-0.046729	4.815811
220.074801	8000.502283	12.534157	-0.046729	4.815820
220.191607	8000.533014	12.539162	-0.046751	4.815828
220.309778	8000.577643	12.544167	-0.046773	4.815841
220.175703	8000.452750	12.549171	-0.046748	4.815805
220.136836	8000.558883	12.554176	-0.046741	4.815836
220.351313	8000.408671	12.559181	-0.046781	4.815791
220.110308	8000.557434	12.564186	-0.046737	4.815836
220.267096	8000.399885	12.569191	-0.046766	4.815789
220.155578	8000.506979	12.574195	-0.046746	4.815821
220.188639	8000.541693	12.579200	-0.046752	4.815831
220.030774	8000.484728	12.584205	-0.046723	4.815815
220.106458	8000.535074	12.589210	-0.046737	4.815829
220.222268	8000.528431	12.594215	-0.046759	4.815827
220.260526	8000.388179	12.599219	-0.046767	4.815786
220.294890	8000.395162	12.604224	-0.046773	4.815788
220.470268	8000.420435	12.609229	-0.046806	4.815794
220.395163	8000.565476	12.614234	-0.046793	4.815837
220.193942	8000.462980	12.619239	-0.046755	4.815808
220.313090	8000.423302	12.624243	-0.046778	4.815796
220.341036	8000.497426	12.629248	-0.046783	4.815817
220.250294	8000.491713	12.634253	-0.046767	4.815816
220.162854	8000.478582	12.639258	-0.046751	4.815813
220.323812	8000.514296	12.644263	-0.046781	4.815822
220.322420	8000.302957	12.649267	-0.046781	4.815760
220.175443	8000.510877	12.654272	-0.046754	4.815822
220.288644	8000.508461	12.659277	-0.046775	4.815821
220.230192	8000.528887	12.664282	-0.046765	4.815827
220.359897	8000.489379	12.669287	-0.046789	4.815815
220.479476	8000.573525	12.674291	-0.046811	4.815839
220.143865	8000.491271	12.679296	-0.046749	4.815816
220.470421	8000.512584	12.684301	-0.046810	4.815821
220.421823	8000.479800	12.689306	-0.046802	4.815812
220.362051	8000.570653	12.694311	-0.046791	4.815838
220.292327	8000.518315	12.699315	-0.046778	4.815823
220.097352	8000.479963	12.704320	-0.046742	4.815813
220.161520	8000.459676	12.709325	-0.046754	4.815807
220.182703	8000.542230	12.714330	-0.046758	4.815831
220.120587	8000.494285	12.719335	-0.046747	4.815817
220.277160	8000.540602	12.724339	-0.046776	4.815830
220.394162	8000.380275	12.729344	-0.046798	4.815783
220.389793	8000.495505	12.734349	-0.046798	4.815816
220.237036	8000.453566	12.739354	-0.046770	4.815805
220.458801	8000.519082	12.744359	-0.046811	4.815823
220.389249	8000.492364	12.749363	-0.046799	4.815815
220.279212	8000.400949	12.754368	-0.046778	4.815789
220.449795	8000.411201	12.759373	-0.046810	4.815791
220.474849	8000.533311	12.764378	-0.046815	4.815827
220.446855	8000.377045	12.769383	-0.046810	4.815781
220.463084	8000.512888	12.774387	-0.046814	4.815821
220.475806	8000.550476	12.779392	-0.046816	4.815832
220.515375	8000.484961	12.784397	-0.046824	4.815813
220.332484	8000.467084	12.789402	-0.046790	4.815808
220.427845	8000.419550	12.794407	-0.046808	4.815794
220.315271	8000.416686	12.799411	-0.046788	4.815793
220.292867	8000.504940	12.804416	-0.046784	4.815819
220.318316	8000.566216	12.809421	-0.046789	4.815837
220.472130	8000.547378	12.814426	-0.046818	4.815831
220.423752	8000.459094	12.819431	-0.046809	4.815805
220.438514	8000.557556	12.824435	-0.046812	4.815834
220.554384	8000.541307	12.829440	-0.046834	4.815829
220.398673	8000.429940	12.834445	-0.046805	4.815797
220.268267	8000.551671	12.839450	-0.046781	4.815833
220.272190	8000.483446	12.844455	-0.046782	4.815813
220.492851	8000.475295	12.849459	-0.046823	4.815810
220.297367	8000.514854	12.854464	-0.046787	4.815822
220.396325	8000.472714	12.859469	-0.046806	4.815809
220.316594	8000.532290	12.864474	-0.046791	4.815827
220.249519	8000.493870	12.869479	-0.046779	4.815816
220.191188	8000.524972	12.874483	-0.046769	4.815826
220.373320	8000.431876	12.879488	-0.046803	4.815798
220.357015	8000.394277	12.884493	-0.046800	4.815787
220.279440	8000.504054	12.889498	-0.046786	4.815819
220.541275	8000.476289	12.894503	-0.046835	4.815810
220.295234	8000.394416	12.899507	-0.046789	4.815787
220.123157	8000.558170	12.904512	-0.046758	4.815836
220.316976	8000.396950	12.909517	-0.046794	4.815788
220.451891	8000.515499	12.914522	-0.046819	4.815822
220.348598	8000.458348	12.919527	-0.046800	4.815805
220.264402	8000.535997	12.924531	-0.046785	4.815828
220.443444	8000.547454	12.929536	-0.046819	4.815831
220.419886	8000.486256	12.934541	-0.046814	4.815813
220.188808	8000.485746	12.939546	-0.046772	4.815814
220.225934	8000.489571	12.944551	-0.046779	4.815815
220.342440	8000.501085	12.949555	-0.046801	4.815818
220.262413	8000.443243	12.954560	-0.046786	4.815801
220.252875	8000.493279	12.959565	-0.046785	4.815816
220.190236	8000.542457	12.964570	-0.046773	4.815831
220.158546	8000.499273	12.969575	-0.046768	4.815818
220.188396	8000.575563	12.974579	-0.046774	4.815840
220.266093	8000.470105	12.979584	-0.046788	4.815809
220.605908	8000.505508	12.984589	-0.046852	4.815818
220.155167	8000.584703	12.989594	-0.046768	4.815843
220.244599	8000.457019	12.994599	-0.046785	4.815805
220.527048	8000.557673	12.999603	-0.046838	4.815833
220.171763	8000.497516	13.004608	-0.046772	4.815818
220.196493	8000.412549	13.009613	-0.046777	4.815793
220.307469	8000.559531	13.014618	-0.046798	4.815835
220.186073	8000.472201	13.019623	-0.046775	4.815810
220.230886	8000.570081	13.024627	-0.046784	4.815838
220.388393	8000.476586	13.029632	-0.046814	4.815810
220.572884	8000.503074	13.034637	-0.046848	4.815817
220.328109	8000.493804	13.039642	-0.046803	4.815816
220.466859	8000.519553	13.044647	-0.046829	4.815823
220.694893	8000.508319	13.049651	-0.046872	4.815818
220.543730	8000.482416	13.054656	-0.046844	4.815811
220.302645	8000.407028	13.059661	-0.046799	4.815790
220.544500	8000.600956	13.064666	-0.046845	4.815846
220.504239	8000.431681	13.069671	-0.046837	4.815797
220.375019	8000.506467	13.074675	-0.046814	4.815819
220.310355	8000.460615	13.079680	-0.046802	4.815806
220.372303	8000.408271	13.084685	-0.046814	4.815790
220.171881	8000.586510	13.089690	-0.046777	4.815843
220.330581	8000.406576	13.094695	-0.046806	4.815790
220.575288	8000.564260	13.099699	-0.046852	4.815835
220.650376	8000.470499	13.104704	-0.046866	4.815807
220.462643	8000.481363	13.109709	-0.046832	4.815811
220.466577	8000.522011	13.114714	-0.046833	4.815823
220.573143	8000.469321	13.119719	-0.046853	4.815807
220.488681	8000.406070	13.124723	-0.046837	4.815789
220.305417	8000.569643	13.129728	-0.046804	4.815838
220.627465	8000.209828	13.134733	-0.046864	4.815731
220.475743	8000.493457	13.139738	-0.046836	4.815815
220.579944	8000.510109	13.144743	-0.046856	4.815819
220.623084	8000.517234	13.149747	-0.046864	4.815821
220.560541	8000.493831	13.154752	-0.046852	4.815814
220.527508	8000.407930	13.159757	-0.046847	4.815789
220.377023	8000.517596	13.164762	-0.046819	4.815822
220.464234	8000.515827	13.169767	-0.046835	4.815821
220.357059	8000.414851	13.174771	-0.046816	4.815792
220.326515	8000.478424	13.179776	-0.046810	4.815811
220.579906	8000.467600	13.184781	-0.046858	4.815807
220.494364	8000.503599	13.189786	-0.046842	4.815818
220.575863	8000.486795	13.194791	-0.046857	4.815812
220.616192	8000.421292	13.199795	-0.046865	4.815793
220.498117	8000.567774	13.204800	-0.046844	4.815836
220.492578	8000.478047	13.209805	-0.046843	4.815810
220.384290	8000.545700	13.214810	-0.046823	4.815830
220.479033	8000.480010	13.219815	-0.046841	4.815811
220.664433	8000.501176	13.224819	-0.046876	4.815816
220.415309	8000.469420	13.229824	-0.046829	4.815808
220.643110	8000.494474	13.234829	-0.046872	4.815814
220.699038	8000.567985	13.239834	-0.046883	4.815835
220.624026	8000.484606	13.244839	-0.046869	4.815811
220.643539	8000.400621	13.249843	-0.046873	4.815787
220.583884	8000.562991	13.254848	-0.046862	4.815834
220.696380	8000.380175	13.259853	-0.046883	4.815780
220.440962	8000.484942	13.264858	-0.046836	4.815812
220.606890	8000.478042	13.269863	-0.046867	4.815809
220.554966	8000.542337	13.274867	-0.046858	4.815828
220.478363	8000.501628	13.279872	-0.046844	4.815817
220.603514	8000.483395	13.284877	-0.046867	4.815811
220.556084	8000.558436	13.289882	-0.046859	4.815833
220.607104	8000.387435	13.294887	-0.046869	4.815783
220.575962	8000.502233	13.299891	-0.046863	4.815817
220.760883	8000.562886	13.304896	-0.046898	4.815833
220.773966	8000.414753	13.309901	-0.046901	4.815790
220.613842	8000.561622	13.314906	-0.046871	4.815834
220.789462	8000.480161	13.319911	-0.046904	4.815809
220.676406	8000.577624	13.324915	-0.046883	4.815838
220.380617	8000.457587	13.329920	-0.046828	4.815804
220.755574	8000.505301	13.334925	-0.046899	4.815817
220.714379	8000.595387	13.339930	-0.046891	4.815843
220.609356	8000.470962	13.344935	-0.046872	4.815807
220.585192	8000.388406	13.349939	-0.046868	4.815783
220.698008	8000.518340	13.354944	-0.046889	4.815821
220.932485	8000.387663	13.359949	-0.046933	4.815781
220.687217	8000.496865	13.364954	-0.046887	4.815814
220.832176	8000.515243	13.369959	-0.046915	4.815819
220.980095	8000.399177	13.374963	-0.046942	4.815784
220.563384	8000.546168	13.379968	-0.046865	4.815829
220.770003	8000.485488	13.384973	-0.046904	4.815811
220.884289	8000.427586	13.389978	-0.046925	4.815793
220.701776	8000.391569	13.394983	-0.046892	4.815784
220.625059	8000.518439	13.399987	-0.046878	4.815821
220.708650	8000.495264	13.404992	-0.046894	4.815814
220.424262	8000.486420	13.409997	-0.046841	4.815813
220.502920	8000.495187	13.415002	-0.046856	4.815815
220.414115	8000.580233	13.420007	-0.046840	4.815840
220.556255	8000.408570	13.425011	-0.046866	4.815789
220.595863	8000.549062	13.430016	-0.046874	4.815830
220.543283	8000.575988	13.435021	-0.046864	4.815838
220.548830	8000.492844	13.440026	-0.046866	4.815814
220.530713	8000.486171	13.445031	-0.046863	4.815812
220.733758	8000.383805	13.450035	-0.046901	4.815781
220.704180	8000.470876	13.455040	-0.046895	4.815807
220.875792	8000.434181	13.460045	-0.046928	4.815795
220.521313	8000.503191	13.465050	-0.046862	4.815817
220.529902	8000.404086	13.470055	-0.046864	4.815788
220.675217	8000.500389	13.475059	-0.046891	4.815815
220.439286	8000.479520	13.480064	-0.046847	4.815810
220.334323	8000.390321	13.485069	-0.046828	4.815785
220.556029	8000.584991	13.490074	-0.046870	4.815841
220.736671	8000.475859	13.495079	-0.046904	4.815808
220.475983	8000.379873	13.500083	-0.046855	4.815781
220.484139	8000.464351	13.505088	-0.046857	4.815806
220.466742	8000.506789	13.510093	-0.046854	4.815818
220.463266	8000.501419	13.515098	-0.046854	4.815817
220.750133	8000.395072	13.520103	-0.046907	4.815784
220.684052	8000.514643	13.525107	-0.046895	4.815819
220.454430	8000.517358	13.530112	-0.046853	4.815821
220.646932	8000.373194	13.535117	-0.046889	4.815778
220.509370	8000.473463	13.540122	-0.046864	4.815808
220.531459	8000.574178	13.545127	-0.046868	4.815838
220.479784	8000.499716	13.550131	-0.046859	4.815816
220.797149	8000.474984	13.555136	-0.046918	4.815807
220.911865	8000.406414	13.560141	-0.046940	4.815787
220.564388	8000.503289	13.565146	-0.046875	4.815817
220.463422	8000.409885	13.570151	-0.046857	4.815790
220.599594	8000.416379	13.575155	-0.046882	4.815791
220.692946	8000.426451	13.580160	-0.046900	4.815793
220.528236	8000.453698	13.585165	-0.046870	4.815802
220.538043	8000.500846	13.590170	-0.046872	4.815816
220.431459	8000.410553	13.595175	-0.046852	4.815790
220.480841	8000.408172	13.600179	-0.046862	4.815789
220.448449	8000.505872	13.605184	-0.046856	4.815818
220.752006	8000.346425	13.610189	-0.046913	4.815770
220.817230	8000.413681	13.615194	-0.046925	4.815789
220.676061	8000.466927	13.620199	-0.046899	4.815805
220.667694	8000.496702	13.625203	-0.046898	4.815814
220.761719	8000.561222	13.630208	-0.046916	4.815833
220.752764	8000.474642	13.635213	-0.046914	4.815807
220.735659	8000.493602	13.640218	-0.046911	4.815813
220.781414	8000.486893	13.645223	-0.046920	4.815811
220.809251	8000.405177	13.650227	-0.046925	4.815787
220.622005	8000.591102	13.655232	-0.046891	4.815842
220.731321	8000.493625	13.660237	-0.046912	4.815813
220.608889	8000.425491	13.665242	-0.046889	4.815793
220.459209	8000.462588	13.670247	-0.046861	4.815805
220.664013	8000.418957	13.675251	-0.046900	4.815791
220.611471	8000.539814	13.680256	-0.046890	4.815827
220.613493	8000.490770	13.685261	-0.046891	4.815813
220.643276	8000.571330	13.690266	-0.046897	4.815836
220.593181	8000.479815	13.695271	-0.046888	4.815809
220.691570	8000.577495	13.700275	-0.046906	4.815838
220.723235	8000.464886	13.705280	-0.046912	4.815804
220.786640	8000.497957	13.710285	-0.046925	4.815814
220.639220	8000.540427	13.715290	-0.046897	4.815827
220.532663	8000.457606	13.720295	-0.046878	4.815803
220.824958	8000.566960	13.725299	-0.046933	4.815834
220.597925	8000.488595	13.730304	-0.046890	4.815812
220.624216	8000.414326	13.735309	-0.046896	4.815790
220.634861	8000.543676	13.740314	-0.046898	4.815828
220.682251	8000.339526	13.745319	-0.046907	4.815768
220.832679	8000.509563	13.750323	-0.046935	4.815817
220.543366	8000.560413	13.755328	-0.046882	4.815833
220.653004	8000.498165	13.760333	-0.046902	4.815814
220.633013	8000.435956	13.765338	-0.046899	4.815796
220.466319	8000.348961	13.770343	-0.046868	4.815772
220.664040	8000.569930	13.775347	-0.046905	4.815835
220.770516	8000.468137	13.780352	-0.046925	4.815805
220.742576	8000.506135	13.785357	-0.046920	4.815816
220.564985	8000.531039	13.790362	-0.046888	4.815824
220.909437	8000.469387	13.795367	-0.046952	4.815805
220.889959	8000.537409	13.800371	-0.046949	4.815825
220.503343	8000.476743	13.805376	-0.046877	4.815809
220.755825	8000.501130	13.810381	-0.046924	4.815815
220.718039	8000.567789	13.815386	-0.046918	4.815834
220.522136	8000.435489	13.820391	-0.046881	4.815797
220.677436	8000.515944	13.825395	-0.046910	4.815819
220.642891	8000.525015	13.830400	-0.046904	4.815822
220.653008	8000.565763	13.835405	-0.046906	4.815834
220.649947	8000.464334	13.840410	-0.046906	4.815804
220.779799	8000.555052	13.845415	-0.046931	4.815830
220.667703	8000.520173	13.850419	-0.046910	4.815821
220.681685	8000.474525	13.855424	-0.046913	4.815807
220.753166	8000.393514	13.860429	-0.046926	4.815783
220.930887	8000.490343	13.865434	-0.046960	4.815811
220.784290	8000.462378	13.870439	-0.046933	4.815803
220.916028	8000.508295	13.875443	-0.046958	4.815816
220.978803	8000.459166	13.880448	-0.046970	4.815801
220.840747	8000.483642	13.885453	-0.046944	4.815809
220.887607	8000.565546	13.890458	-0.046953	4.815833
220.814645	8000.457649	13.895463	-0.046940	4.815802
220.953113	8000.594405	13.900467	-0.046966	4.815841
220.848247	8000.455037	13.905472	-0.046947	4.815801
220.900219	8000.491125	13.910477	-0.046957	4.815811
220.655702	8000.475453	13.915482	-0.046911	4.815808
220.853957	8000.558738	13.920487	-0.046948	4.815831
220.871521	8000.485395	13.925491	-0.046952	4.815809
220.853222	8000.538492	13.930496	-0.046949	4.815825
220.770463	8000.467796	13.935501	-0.046934	4.815805
220.661261	8000.541839	13.940506	-0.046914	4.815827
220.739193	8000.406496	13.945511	-0.046928	4.815787
220.959364	8000.485865	13.950515	-0.046970	4.815809
220.794707	8000.543000	13.955520	-0.046939	4.815827
220.912683	8000.508640	13.960525	-0.046962	4.815816
221.104258	8000.546986	13.965530	-0.046998	4.815826
220.986721	8000.472525	13.970535	-0.046976	4.815805
221.005816	8000.485666	13.975539	-0.046980	4.815809
220.790834	8000.564403	13.980544	-0.046940	4.815833
220.972046	8000.479830	13.985549	-0.046974	4.815807
220.686561	8000.499787	13.990554	-0.046921	4.815814
220.821267	8000.566033	13.995559	-0.046946	4.815833
220.790318	8000.490838	14.000563	-0.046941	4.815811
220.716987	8000.563326	14.005568	-0.046928	4.815833
220.839958	8000.351858	14.010573	-0.046951	4.815770
220.750254	8000.461441	14.015578	-0.046934	4.815803
220.770124	8000.477796	14.020583	-0.046938	4.815808
220.933704	8000.385466	14.025587	-0.046969	4.815780
220.940649	8000.561724	14.030592	-0.046971	4.815831
220.834275	8000.538679	14.035597	-0.046951	4.815825
220.841312	8000.464098	14.040602	-0.046953	4.815803
220.990512	8000.558331	14.045607	-0.046981	4.815830
221.175477	8000.479155	14.050611	-0.047015	4.815806
221.009667	8000.536272	14.055616	-0.046985	4.815823
220.982692	8000.433388	14.060621	-0.046980	4.815793
221.069162	8000.553293	14.065626	-0.046996	4.815828
220.902435	8000.498316	14.070631	-0.046966	4.815813
220.852621	8000.513545	14.075635	-0.046957	4.815818
220.993688	8000.558547	14.080640	-0.046983	4.815830
220.985938	8000.464513	14.085645	-0.046982	4.815803
220.888555	8000.552624	14.090650	-0.046964	4.815829
220.877796	8000.464946	14.095655	-0.046962	4.815803
221.046740	8000.501858	14.100659	-0.046994	4.815813
220.825868	8000.482299	14.105664	-0.046953	4.815808
220.983075	8000.354641	14.110669	-0.046983	4.815770
220.996842	8000.512863	14.115674	-0.046986	4.815817
220.907919	8000.459146	14.120679	-0.046969	4.815801
221.011121	8000.499265	14.125683	-0.046989	4.815813
220.984589	8000.554365	14.130688	-0.046984	4.815829
220.923966	8000.573688	14.135693	-0.046973	4.815835
220.888391	8000.450385	14.140698	-0.046967	4.815799
220.895724	8000.515638	14.145703	-0.046968	4.815818
221.000389	8000.467186	14.150707	-0.046988	4.815803
220.765913	8000.471957	14.155712	-0.046945	4.815806
220.911601	8000.386810	14.160717	-0.046972	4.815780
220.883685	8000.493122	14.165722	-0.046967	4.815811
221.101254	8000.529754	14.170727	-0.047008	4.815821
220.786717	8000.481994	14.175731	-0.046950	4.815808
221.018471	8000.538069	14.180736	-0.046993	4.815824
221.047999	8000.571660	14.185741	-0.046999	4.815833
220.955083	8000.468776	14.190746	-0.046982	4.815804
220.965892	8000.476446	14.195751	-0.046984	4.815806
221.046224	8000.501252	14.200755	-0.046999	4.815813
220.945495	8000.564759	14.205760	-0.046981	4.815832
221.106412	8000.574857	14.210765	-0.047011	4.815834
221.113018	8000.481055	14.215770	-0.047013	4.815807
221.076197	8000.474078	14.220775	-0.047006	4.815805
221.052010	8000.405396	14.225779	-0.047002	4.815785
220.834772	8000.492636	14.230784	-0.046962	4.815811
221.059867	8000.400233	14.235789	-0.047004	4.815783
220.856679	8000.552812	14.240794	-0.046966	4.815829
220.822960	8000.423134	14.245799	-0.046960	4.815791
220.913728	7999.539772	14.250803	-0.046977	4.815532

220.854651	7996.235745	14.255808	-0.046964	4.814566
220.988796	7990.646036	14.260813	-0.046986	4.812930
221.078434	7983.902614	14.265818	-0.046998	4.810955
220.899096	7976.626935	14.270823	-0.046960	4.808825
221.027403	7969.037548	14.275827	-0.046979	4.806601
220.915765	7961.237140	14.280832	-0.046954	4.804315
220.812881	7953.405502	14.285837	-0.046930	4.802019
220.693989	7945.394441	14.290842	-0.046903	4.799669
220.545568	7937.436899	14.295847	-0.046870	4.797334
220.849678	7929.454765	14.300851	-0.046922	4.794988
220.752712	7921.399540	14.305856	-0.046899	4.792622
220.694541	7913.367995	14.310861	-0.046883	4.790261
220.544140	7905.377364	14.315866	-0.046850	4.787912
220.497604	7897.404869	14.320871	-0.046837	4.785566
220.410955	7889.470753	14.325875	-0.046815	4.783230
220.328420	7881.424049	14.330880	-0.046795	4.780860
220.572029	7873.384586	14.335885	-0.046836	4.778490
220.388450	7865.449374	14.340890	-0.046796	4.776151
220.397449	7857.343879	14.345895	-0.046793	4.773760
220.352837	7849.427904	14.350899	-0.046780	4.771424
220.306852	7841.387915	14.355904	-0.046766	4.769050
220.117129	7833.404093	14.360909	-0.046726	4.766692
220.175781	7825.371301	14.365914	-0.046732	4.764317
220.235347	7817.414279	14.370919	-0.046738	4.761964
220.140942	7809.398213	14.375923	-0.046716	4.759592
219.831610	7801.440683	14.380928	-0.046653	4.757238
219.954500	7793.392981	14.385933	-0.046671	4.754854
219.939068	7785.328800	14.390938	-0.046663	4.752464
219.646732	7777.276234	14.395943	-0.046604	4.750078
219.731901	7769.324426	14.400947	-0.046615	4.747719
219.654554	7761.314909	14.405952	-0.046595	4.745342
219.743891	7753.362650	14.410957	-0.046607	4.742980
219.579829	7745.360309	14.415962	-0.046572	4.740603
219.681592	7737.345757	14.420967	-0.046586	4.738221
219.655364	7729.357065	14.425971	-0.046576	4.735846
219.513554	7721.322005	14.430976	-0.046544	4.733455
219.616124	7713.271301	14.435981	-0.046559	4.731059
219.675525	7705.316480	14.440986	-0.046565	4.728689
219.649769	7697.305172	14.445991	-0.046555	4.726302
219.484977	7689.309292	14.450995	-0.046519	4.723919
219.620869	7681.349358	14.456000	-0.046540	4.721544
219.455687	7673.337559	14.461005	-0.046504	4.719154
219.124370	7665.396499	14.466010	-0.046437	4.716784
219.216145	7657.331247	14.471015	-0.046450	4.714374
219.547484	7649.324144	14.476019	-0.046506	4.711980
219.204766	7641.264804	14.481024	-0.046438	4.709571
219.201279	7633.358252	14.486029	-0.046432	4.707205
219.133867	7625.294655	14.491034	-0.046414	4.704792
219.071969	7617.280080	14.496039	-0.046398	4.702391
218.970073	7609.323525	14.501043	-0.046374	4.700007
219.145604	7601.333299	14.506048	-0.046402	4.697612
219.313309	7593.296054	14.511053	-0.046428	4.695201
219.151976	7585.322226	14.516058	-0.046393	4.692808
218.981959	7577.254772	14.521063	-0.046356	4.690386
219.043534	7569.292627	14.526067	-0.046363	4.687994
218.749353	7561.250522	14.531072	-0.046303	4.685577
218.808259	7553.317327	14.536077	-0.046309	4.683191
218.803139	7545.293431	14.541082	-0.046303	4.680777
218.548692	7537.283852	14.546087	-0.046251	4.678366
218.655755	7529.326864	14.551091	-0.046266	4.675969
218.589434	7521.213626	14.556096	-0.046249	4.673524
218.673034	7513.148801	14.561101	-0.046259	4.671093
218.479920	7505.183217	14.566106	-0.046218	4.668690
218.552526	7497.190818	14.571111	-0.046227	4.666278
218.547645	7489.233246	14.576115	-0.046221	4.663875
218.204485	7481.247574	14.581120	-0.046152	4.661462
218.564251	7473.225209	14.586125	-0.046214	4.659037
218.275899	7465.261563	14.591130	-0.046156	4.656628
218.329100	7457.191794	14.596135	-0.046161	4.654186
218.335495	7449.253946	14.601139	-0.046157	4.651783
218.174764	7441.198184	14.606144	-0.046122	4.649343
218.258261	7433.252357	14.611149	-0.046133	4.646935
218.072023	7425.223560	14.616154	-0.046093	4.644500
218.076382	7417.261168	14.621159	-0.046089	4.642084
218.137645	7409.268075	14.626163	-0.046095	4.639658
218.148986	7401.219460	14.631168	-0.046093	4.637213
218.108148	7393.176043	14.636173	-0.046080	4.634769
218.178116	7385.188363	14.641178	-0.046088	4.632341
218.175382	7377.156551	14.646183	-0.046083	4.629897
218.069500	7369.216061	14.651187	-0.046058	4.627481
218.078145	7361.181454	14.656192	-0.046055	4.625034
217.915824	7353.220675	14.661197	-0.046020	4.622608
217.800684	7345.223206	14.666202	-0.045993	4.620170
217.903608	7337.168638	14.671207	-0.046007	4.617714
218.044267	7329.194007	14.676211	-0.046029	4.615280
217.799157	7321.166392	14.681216	-0.045978	4.612829
217.790769	7313.148148	14.686221	-0.045971	4.610379
217.798484	7305.214835	14.691226	-0.045968	4.607955
217.809137	7297.175476	14.696231	-0.045965	4.605496
217.762522	7289.195556	14.701235	-0.045951	4.603054
217.774717	7281.164770	14.706240	-0.045949	4.600596
217.584204	7273.204802	14.711245	-0.045908	4.598157
217.533921	7265.194935	14.716250	-0.045894	4.595703
217.398099	7257.118279	14.721255	-0.045864	4.593226
217.301979	7249.090723	14.726259	-0.045841	4.590763
217.217640	7241.103081	14.731264	-0.045820	4.588311
217.290350	7233.103112	14.736269	-0.045829	4.585854
217.257604	7225.150343	14.741274	-0.045818	4.583410
217.362637	7217.122272	14.746279	-0.045832	4.580942
217.222283	7209.165174	14.751283	-0.045801	4.578494
217.039346	7201.136476	14.756288	-0.045762	4.576022
217.123792	7193.136631	14.761293	-0.045773	4.573559
217.126086	7185.113002	14.766298	-0.045769	4.571087
217.108852	7177.106955	14.771303	-0.045760	4.568618
216.963965	7169.135097	14.776307	-0.045729	4.566159
216.925352	7161.129739	14.781312	-0.045716	4.563688
217.057851	7153.158321	14.786317	-0.045736	4.561227
216.940067	7145.175121	14.791322	-0.045709	4.558760
216.907356	7137.152479	14.796327	-0.045698	4.556280
216.806004	7129.137591	14.801331	-0.045674	4.553801
216.692280	7121.094905	14.806336	-0.045648	4.551312
216.609896	7113.109928	14.811341	-0.045628	4.548839
216.680192	7105.118419	14.816346	-0.045636	4.546363
216.570350	7097.066822	14.821351	-0.045611	4.543867
216.597899	7089.177891	14.826355	-0.045611	4.541421
216.556271	7081.105547	14.831360	-0.045598	4.538916
216.471261	7073.189744	14.836365	-0.045578	4.536458
216.646120	7065.121873	14.841370	-0.045605	4.533952
216.603556	7057.084952	14.846375	-0.045592	4.531453
216.669493	7049.088876	14.851379	-0.045600	4.528967
216.344446	7041.122997	14.856384	-0.045534	4.526487
216.311511	7033.119405	14.861389	-0.045523	4.523995
216.316379	7025.176070	14.866394	-0.045519	4.521521
216.059782	7017.121924	14.871399	-0.045466	4.519010
216.410493	7009.171697	14.876403	-0.045527	4.516531
216.249371	7001.077769	14.881408	-0.045492	4.514005
216.137244	6993.035025	14.886413	-0.045466	4.511494
216.072748	6985.044369	14.891418	-0.045449	4.508997
216.046710	6977.038868	14.896423	-0.045439	4.506495
215.944713	6969.073430	14.901427	-0.045415	4.504004
215.638536	6961.060417	14.906432	-0.045353	4.501496
215.874960	6953.067955	14.911437	-0.045392	4.498994
215.857858	6945.099166	14.916442	-0.045384	4.496498
215.911071	6937.018634	14.921447	-0.045389	4.493965
215.945744	6929.070213	14.926451	-0.045391	4.491472
216.048927	6921.038981	14.931456	-0.045405	4.488953
215.824277	6913.079173	14.936461	-0.045358	4.486453
215.926615	6905.079783	14.941466	-0.045372	4.483940
215.959812	6897.051809	14.946471	-0.045373	4.481417
215.917582	6889.091684	14.951475	-0.045361	4.478913
215.565042	6881.098754	14.956480	-0.045290	4.476397
215.733924	6873.076915	14.961485	-0.045317	4.473872
215.729903	6865.053575	14.966490	-0.045311	4.471344
215.434668	6857.028227	14.971495	-0.045251	4.468814
215.504407	6849.053753	14.976499	-0.045259	4.466299
215.453940	6841.036715	14.981504	-0.045245	4.463769
215.355652	6833.044597	14.986509	-0.045221	4.461245
215.416915	6825.044224	14.991514	-0.045228	4.458718
215.389039	6817.009986	14.996519	-0.045218	4.456178
215.521323	6809.017792	15.001523	-0.045237	4.453651
215.229572	6801.000034	15.006528	-0.045178	4.451112
215.301915	6793.022637	15.011533	-0.045187	4.448587
215.314237	6785.045618	15.016538	-0.045184	4.446059
215.195955	6776.995143	15.021543	-0.045157	4.443507
215.214177	6769.053759	15.026547	-0.045155	4.440988
215.243555	6761.016417	15.031552	-0.045156	4.438437
215.005688	6753.060167	15.036557	-0.045107	4.435910
215.084296	6745.006811	15.041562	-0.045116	4.433351
215.097233	6736.936445	15.046567	-0.045114	4.430786
215.004233	6728.960608	15.051571	-0.045092	4.428248
214.935850	6720.972352	15.056576	-0.045074	4.425705
214.667492	6712.970158	15.061581	-0.045019	4.423155
214.814197	6704.982063	15.066586	-0.045041	4.420611
214.487381	6696.967620	15.071591	-0.044976	4.418054
214.556664	6689.026140	15.076595	-0.044984	4.415521
214.540041	6680.942910	15.081600	-0.044976	4.412940
214.718168	6672.974670	15.086605	-0.045004	4.410396
214.500475	6665.010517	15.091610	-0.044958	4.407850
214.522524	6656.933922	15.096615	-0.044957	4.405267
214.547082	6649.016146	15.101619	-0.044957	4.402734
214.493245	6640.981396	15.106624	-0.044942	4.400162
214.551830	6633.035215	15.111629	-0.044948	4.397617
214.424575	6625.025711	15.116634	-0.044919	4.395049
214.492618	6616.944577	15.121639	-0.044927	4.392457
214.271159	6608.986083	15.126643	-0.044881	4.389902
214.214165	6600.992470	15.131648	-0.044865	4.387335
214.214086	6592.965630	15.136653	-0.044860	4.384757
213.934104	6585.035963	15.141658	-0.044803	4.382206
213.925432	6576.978959	15.146663	-0.044797	4.379614
214.113020	6569.069546	15.151667	-0.044827	4.377070
213.889327	6561.030835	15.156672	-0.044780	4.374480
214.180501	6552.979526	15.161677	-0.044830	4.371887
214.019471	6544.949241	15.166682	-0.044795	4.369297
213.837844	6536.980300	15.171687	-0.044756	4.366726
213.770603	6528.987804	15.176691	-0.044738	4.364145
213.915888	6521.016190	15.181696	-0.044760	4.361571
213.901315	6513.006044	15.186701	-0.044753	4.358983
213.960867	6505.045515	15.191706	-0.044759	4.356409
213.987414	6496.948544	15.196711	-0.044759	4.353789
213.972879	6488.890058	15.201715	-0.044751	4.351180
213.763806	6480.918465	15.206720	-0.044707	4.348596
213.611261	6472.926453	15.211725	-0.044674	4.346005
213.720267	6464.960732	15.216730	-0.044689	4.343422
213.599121	6456.957463	15.221735	-0.044662	4.340824
213.686087	6448.994002	15.226739	-0.044673	4.338239
213.586316	6440.961480	15.231744	-0.044650	4.335628
213.622198	6432.959693	15.236749	-0.044651	4.333027
213.399316	6424.958789	15.241754	-0.044605	4.330422
213.321342	6416.933698	15.246759	-0.044585	4.327809
213.584225	6408.949000	15.251763	-0.044629	4.325211
213.527811	6400.969492	15.256768	-0.044614	4.322610
213.544578	6392.987412	15.261773	-0.044612	4.320007
213.386090	6385.046680	15.266778	-0.044578	4.317415
213.256419	6376.934232	15.271783	-0.044549	4.314765
213.477824	6368.936151	15.276787	-0.044585	4.312154
213.374431	6360.905592	15.281792	-0.044561	4.309528
213.315470	6352.935220	15.286797	-0.044545	4.306920
213.239164	6344.912905	15.291802	-0.044526	4.304294
213.112662	6336.957725	15.296807	-0.044497	4.301688
213.212989	6328.934296	15.301811	-0.044511	4.299060
213.051825	6320.957356	15.306816	-0.044476	4.296443
212.880549	6312.942792	15.311821	-0.044439	4.293812
212.969910	6304.893464	15.316826	-0.044451	4.291170
213.063986	6296.882200	15.321831	-0.044463	4.288539
212.887840	6288.933915	15.326835	-0.044426	4.285925
212.791423	6280.931594	15.331840	-0.044403	4.283292
212.874903	6272.945751	15.336845	-0.044413	4.280665
212.831802	6264.957628	15.341850	-0.044400	4.278034
212.748800	6256.947066	15.346855	-0.044380	4.275394
212.667963	6248.916825	15.351859	-0.044360	4.272745
212.508569	6240.875704	15.356864	-0.044325	4.270091
212.565560	6232.890623	15.361869	-0.044331	4.267455
212.624137	6224.901914	15.366874	-0.044337	4.264817
212.495233	6216.892031	15.371879	-0.044308	4.262168
212.491341	6208.921535	15.376883	-0.044302	4.259532
212.409577	6200.901530	15.381888	-0.044282	4.256877
212.435864	6192.901498	15.386893	-0.044282	4.254228
212.406460	6184.914584	15.391898	-0.044272	4.251581
212.332328	6176.884966	15.396903	-0.044253	4.248918
212.510396	6168.918229	15.401907	-0.044281	4.246276
212.375592	6160.939868	15.406912	-0.044251	4.243627
212.186873	6152.931449	15.411917	-0.044211	4.240964
212.202060	6144.981437	15.416922	-0.044209	4.238322
212.324852	6136.916920	15.421927	-0.044227	4.235641
212.269294	6128.969560	15.426931	-0.044212	4.232995
211.903464	6120.919147	15.431936	-0.044139	4.230311
212.043511	6112.932129	15.436941	-0.044160	4.227650
212.258986	6104.899179	15.441946	-0.044195	4.224974
212.049742	6096.954084	15.446951	-0.044151	4.222321
212.003037	6088.947490	15.451955	-0.044137	4.219647
211.963068	6080.962609	15.456960	-0.044125	4.216979
211.899054	6072.938725	15.461965	-0.044108	4.214296
211.946891	6064.949209	15.466970	-0.044112	4.211624
211.769971	6056.938120	15.471975	-0.044074	4.208940
211.744809	6048.944279	15.476979	-0.044065	4.206263
211.551940	6040.901189	15.481984	-0.044024	4.203565
211.677639	6032.978965	15.486989	-0.044042	4.200909
211.510046	6024.975191	15.491994	-0.044006	4.198222
211.313268	6016.948734	15.496999	-0.043964	4.195524
211.594223	6008.823068	15.502003	-0.044012	4.192797
211.590082	6000.773953	15.507008	-0.044006	4.190090
211.491071	5992.846290	15.512013	-0.043983	4.187422
211.269390	5984.884155	15.517018	-0.043936	4.184739
211.475227	5976.910428	15.522023	-0.043970	4.182055
211.466075	5968.893284	15.527027	-0.043963	4.179352
211.102795	5960.937495	15.532032	-0.043891	4.176665
211.040751	5952.919605	15.537037	-0.043874	4.173957
211.113636	5944.884865	15.542042	-0.043883	4.171244
211.131592	5936.892272	15.547047	-0.043881	4.168543
211.122234	5928.896560	15.552051	-0.043874	4.165839
210.994478	5920.887959	15.557056	-0.043846	4.163127
210.821519	5912.927660	15.562061	-0.043809	4.160430
210.815144	5904.918037	15.567066	-0.043802	4.157715
210.809244	5896.892468	15.572071	-0.043796	4.154994
210.639385	5888.907325	15.577075	-0.043760	4.152282
210.702876	5880.846665	15.582080	-0.043767	4.149546
210.872402	5872.880337	15.587085	-0.043793	4.146842
210.962548	5864.861374	15.592090	-0.043805	4.144116
210.695679	5856.905349	15.597095	-0.043751	4.141407
210.786821	5848.908797	15.602099	-0.043763	4.138685
210.699556	5840.903755	15.607104	-0.043741	4.135957
210.553874	5832.889676	15.612109	-0.043709	4.133224
210.349495	5824.886766	15.617114	-0.043666	4.130491
210.585773	5816.875831	15.622119	-0.043705	4.127760
210.417410	5808.874970	15.627123	-0.043669	4.125025
210.189258	5800.889924	15.632128	-0.043622	4.122293
210.177097	5792.886716	15.637133	-0.043614	4.119556
210.324502	5784.945789	15.642138	-0.043637	4.116840
210.313614	5776.878397	15.647143	-0.043630	4.114077
210.146212	5768.887013	15.652147	-0.043594	4.111336
210.118331	5760.876620	15.657152	-0.043584	4.108589
210.137551	5752.859799	15.662157	-0.043582	4.105838
210.137404	5744.897263	15.667162	-0.043577	4.103104
210.129165	5736.911289	15.672167	-0.043571	4.100359
210.034642	5728.921312	15.677171	-0.043548	4.097611
210.067005	5720.891886	15.682176	-0.043549	4.094848
210.123587	5712.874175	15.687181	-0.043555	4.092089
210.150281	5704.900170	15.692186	-0.043555	4.089342
209.928576	5696.929579	15.697191	-0.043509	4.086590
209.909474	5688.941021	15.702195	-0.043500	4.083834
209.766104	5680.924869	15.707200	-0.043469	4.081064
209.869442	5672.939553	15.712205	-0.043483	4.078307
209.536132	5664.998878	15.717210	-0.043416	4.075557
209.490577	5656.925748	15.722215	-0.043403	4.072764
209.609101	5648.935341	15.727219	-0.043420	4.069999
209.475225	5640.916504	15.732224	-0.043390	4.067219
209.531061	5632.909817	15.737229	-0.043395	4.064444
209.553428	5624.959445	15.742234	-0.043395	4.061687
209.562957	5616.904421	15.747239	-0.043391	4.058891
209.327883	5608.981042	15.752243	-0.043343	4.056135
209.511821	5600.931583	15.757248	-0.043372	4.053340
209.350534	5592.907516	15.762253	-0.043337	4.050546
209.141662	5584.968173	15.767258	-0.043293	4.047779
209.303510	5576.897658	15.772263	-0.043318	4.044970
209.317849	5568.980442	15.777267	-0.043316	4.042211
209.087751	5560.915375	15.782272	-0.043268	4.039394
209.157580	5552.967403	15.787277	-0.043276	4.036621
209.347500	5544.923185	15.792282	-0.043307	4.033814
208.977897	5536.820402	15.797287	-0.043233	4.030976
209.032660	5528.843267	15.802291	-0.043238	4.028186
208.769001	5520.875786	15.807296	-0.043184	4.025394
208.855739	5512.917240	15.812301	-0.043195	4.022607
208.709387	5504.929965	15.817306	-0.043163	4.019805
208.603219	5496.928749	15.822311	-0.043138	4.016997
208.998561	5488.921485	15.827315	-0.043207	4.014192
208.716092	5480.894040	15.832320	-0.043150	4.011368
208.699486	5472.895928	15.837325	-0.043142	4.008557
208.705242	5464.930823	15.842330	-0.043138	4.005755
208.720926	5456.906122	15.847335	-0.043136	4.002930
208.749400	5448.917512	15.852339	-0.043136	4.000117
208.574990	5440.937602	15.857344	-0.043099	3.997301
208.459539	5432.946529	15.862349	-0.043072	3.994480
208.404604	5424.933609	15.867354	-0.043057	3.991651
208.183312	5416.889935	15.872359	-0.043011	3.988806
208.366330	5408.931283	15.877363	-0.043040	3.985995
208.189220	5400.936773	15.882368	-0.043002	3.983164
207.983320	5392.919405	15.887373	-0.042959	3.980323
208.216301	5384.952371	15.892378	-0.042997	3.977504
208.143960	5376.919943	15.897383	-0.042979	3.974655
208.094537	5368.941486	15.902387	-0.042965	3.971824
208.296169	5360.918973	15.907392	-0.042997	3.968979
208.187295	5352.957409	15.912397	-0.042972	3.966149
208.031492	5344.975746	15.917402	-0.042938	3.963308
207.745758	5336.975448	15.922407	-0.042880	3.960457
208.017192	5329.010136	15.927411	-0.042926	3.957626
207.806697	5320.988025	15.932416	-0.042881	3.954764
207.826021	5312.926456	15.937421	-0.042880	3.951890
207.912779	5304.940036	15.942426	-0.042891	3.949042
207.783274	5296.944650	15.947431	-0.042862	3.946184
207.653604	5288.989184	15.952435	-0.042833	3.943339
207.622852	5280.983122	15.957440	-0.042822	3.940476
207.595625	5272.987956	15.962445	-0.042812	3.937614
207.714429	5264.962560	15.967450	-0.042830	3.934742
207.588047	5256.965737	15.972455	-0.042801	3.931874
207.703488	5248.965234	15.977459	-0.042818	3.929007
207.476447	5240.977418	15.982464	-0.042770	3.926136
207.468076	5232.999215	15.987469	-0.042764	3.923270
207.360315	5225.026708	15.992474	-0.042739	3.920402
207.365210	5217.023088	15.997479	-0.042735	3.917524
207.266958	5209.013312	16.002483	-0.042712	3.914639
207.255422	5200.973831	16.007488	-0.042705	3.911742
207.276897	5192.971504	16.012493	-0.042704	3.908858
207.394006	5184.996065	16.017498	-0.042721	3.905983
207.139459	5176.977541	16.022503	-0.042668	3.903083
207.345177	5169.015292	16.027507	-0.042702	3.900210
207.116604	5161.038479	16.032512	-0.042654	3.897322
207.029506	5152.978290	16.037517	-0.042633	3.894404
207.040539	5145.025000	16.042522	-0.042630	3.891524
206.976599	5136.935176	16.047527	-0.042613	3.888591
206.900839	5128.981201	16.052531	-0.042594	3.885705
206.783595	5121.000996	16.057536	-0.042567	3.882807
206.722625	5113.005741	16.062541	-0.042551	3.879902
206.725699	5105.050835	16.067546	-0.042547	3.877010
206.672219	5096.989099	16.072551	-0.042532	3.874077
206.674774	5088.763282	16.077555	-0.042527	3.871083
206.670203	5080.837198	16.082560	-0.042521	3.868195
206.540978	5072.874204	16.087565	-0.042492	3.865289
206.580303	5064.981578	16.092570	-0.042495	3.862411
206.594507	5056.938081	16.097575	-0.042493	3.859474
206.425293	5049.000515	16.102579	-0.042456	3.856570
206.411275	5040.996397	16.107584	-0.042449	3.853643
206.756551	5032.951954	16.112589	-0.042508	3.850706
206.796516	5024.966334	16.117594	-0.042510	3.847782
206.268558	5016.979410	16.122599	-0.042407	3.844844
206.280874	5009.056098	16.127603	-0.042405	3.841938
206.303717	5001.044668	16.132608	-0.042404	3.838998
206.067084	4993.072743	16.137613	-0.042355	3.836065
206.140618	4985.046970	16.142618	-0.042364	3.833116
206.380746	4976.999197	16.147623	-0.042403	3.830160
206.245068	4969.038350	16.152627	-0.042373	3.827226
206.026091	4961.014769	16.157632	-0.042327	3.824264
206.140986	4953.073069	16.162637	-0.042344	3.821338
206.064768	4945.100245	16.167642	-0.042325	3.818394
206.025898	4937.078213	16.172647	-0.042313	3.815430
206.119646	4929.070770	16.177651	-0.042325	3.812473
206.017101	4921.067456	16.182656	-0.042301	3.809510
205.976569	4913.033914	16.187661	-0.042289	3.806535
205.815581	4905.103875	16.192666	-0.042254	3.803593
205.765161	4897.080951	16.197671	-0.042239	3.800617
205.752230	4889.140336	16.202675	-0.042232	3.797671
205.640739	4881.103335	16.207680	-0.042206	3.794683
205.556569	4873.097121	16.212685	-0.042186	3.791706
205.516383	4865.069444	16.217690	-0.042173	3.788719
205.265504	4857.073310	16.222695	-0.042122	3.785737
205.392398	4849.079330	16.227699	-0.042140	3.782762
205.377004	4841.056639	16.232704	-0.042132	3.779770
205.458873	4833.104687	16.237709	-0.042143	3.776805
205.344227	4825.108189	16.242714	-0.042117	3.773816
205.162116	4817.060393	16.247719	-0.042078	3.770804
205.275227	4809.082029	16.252723	-0.042094	3.767823
205.139504	4801.089321	16.257728	-0.042064	3.764828
205.177235	4793.113212	16.262733	-0.042066	3.761841
205.333851	4785.115293	16.267738	-0.042090	3.758846
204.906509	4777.138984	16.272743	-0.042005	3.755843
205.010548	4769.118019	16.277747	-0.042020	3.752834
204.900022	4761.096863	16.282752	-0.041994	3.749817
205.010415	4753.079222	16.287757	-0.042010	3.746803
204.916048	4745.104843	16.292762	-0.041987	3.743799
204.787691	4737.118335	16.297767	-0.041959	3.740788
204.969848	4729.128703	16.302771	-0.041987	3.737780
204.724377	4721.144317	16.307776	-0.041937	3.734761
204.773697	4713.113117	16.312781	-0.041941	3.731729
205.002848	4705.102598	16.317786	-0.041979	3.728707
204.675581	4697.142191	16.322791	-0.041913	3.725688
204.839370	4689.183373	16.327795	-0.041939	3.722679
204.771750	4681.164218	16.332800	-0.041921	3.719639
204.819258	4673.216673	16.337805	-0.041925	3.716627
204.680252	4665.181508	16.342810	-0.041894	3.713574
204.518969	4657.088726	16.347815	-0.041859	3.710496
204.719984	4649.122893	16.352819	-0.041892	3.707473
204.446861	4641.127071	16.357824	-0.041836	3.704425
204.226946	4633.199233	16.362829	-0.041790	3.701401
204.220405	4625.177198	16.367834	-0.041784	3.698344
204.045584	4617.202312	16.372839	-0.041746	3.695298
204.205320	4609.203873	16.377843	-0.041771	3.692249
204.222605	4601.200963	16.382848	-0.041769	3.689192
204.071594	4593.219914	16.387853	-0.041736	3.686137
204.041577	4585.243224	16.392858	-0.041726	3.683084
204.032573	4577.221244	16.397863	-0.041719	3.680012
204.006262	4569.271451	16.402867	-0.041709	3.676964
203.946206	4561.239414	16.407872	-0.041693	3.673881
203.921409	4553.201214	16.412877	-0.041684	3.670795
204.031861	4545.226458	16.417882	-0.041699	3.667733
203.899353	4537.198464	16.422887	-0.041670	3.664642
203.905818	4529.248153	16.427891	-0.041666	3.661582
203.883959	4521.261050	16.432896	-0.041657	3.658505
203.891488	4513.246302	16.437901	-0.041653	3.655415
203.745601	4505.245587	16.442906	-0.041621	3.652324
203.806809	4497.201154	16.447911	-0.041628	3.649219
203.809669	4489.270092	16.452915	-0.041623	3.646154
203.813827	4481.260108	16.457920	-0.041619	3.643055
203.443942	4473.282805	16.462925	-0.041545	3.639956
203.611349	4465.330775	16.467930	-0.041572	3.636879
203.593354	4457.272778	16.472935	-0.041563	3.633754
203.557963	4449.237411	16.477939	-0.041552	3.630633
203.341916	4441.252127	16.482944	-0.041506	3.627525
203.335581	4433.230996	16.487949	-0.041500	3.624406
203.283399	4425.329854	16.492954	-0.041486	3.621330
203.487412	4417.293214	16.497959	-0.041519	3.618205
203.581341	4409.308834	16.502963	-0.041531	3.615095
203.365627	4401.333243	16.507968	-0.041486	3.611977
203.229201	4393.309463	16.512973	-0.041456	3.608839
203.190416	4385.345645	16.517978	-0.041444	3.605725
203.018741	4377.355152	16.522983	-0.041407	3.602595
202.848600	4369.360419	16.527987	-0.041370	3.599460
202.799723	4361.360834	16.532992	-0.041356	3.596323
203.091095	4353.342946	16.537997	-0.041405	3.593187
202.958522	4345.363353	16.543002	-0.041376	3.590050
202.844540	4337.356890	16.548007	-0.041350	3.586901
202.731679	4329.374096	16.553011	-0.041324	3.583758
202.709590	4321.378273	16.558016	-0.041315	3.580611
202.656852	4313.433716	16.563021	-0.041300	3.577479
202.662599	4305.426175	16.568026	-0.041296	3.574322
202.633989	4297.421908	16.573031	-0.041286	3.571162
202.543980	4289.400031	16.578035	-0.041264	3.567991
202.516498	4281.402819	16.583040	-0.041254	3.564828
202.487969	4273.442765	16.588045	-0.041244	3.561677
202.585049	4265.448940	16.593050	-0.041257	3.558514
202.505029	4257.417102	16.598055	-0.041237	3.555328
202.663203	4249.355870	16.603059	-0.041262	3.552134
202.522368	4241.349318	16.608064	-0.041230	3.548950
202.316011	4233.365137	16.613069	-0.041187	3.545771
202.372112	4225.402222	16.618074	-0.041193	3.542604
202.250835	4217.391590	16.623079	-0.041165	3.539411
202.061796	4209.466963	16.628083	-0.041125	3.536247
202.108221	4201.424522	16.633088	-0.041129	3.533040
202.260286	4193.394634	16.638093	-0.041152	3.529838
202.193871	4185.435443	16.643098	-0.041135	3.526655
201.891355	4177.432057	16.648103	-0.041073	3.523444
202.004317	4169.473695	16.653107	-0.041089	3.520262
201.916208	4161.492738	16.658112	-0.041068	3.517061
201.839725	4153.468408	16.663117	-0.041049	3.513840
201.852411	4145.477247	16.668122	-0.041046	3.510632
201.776775	4137.465269	16.673127	-0.041027	3.507410
201.925759	4129.477430	16.678131	-0.041050	3.504202
201.820338	4121.517373	16.683136	-0.041026	3.500994
201.726339	4113.535122	16.688141	-0.041003	3.497774
201.831969	4105.560937	16.693146	-0.041018	3.494562
201.693567	4097.532741	16.698151	-0.040987	3.491316
201.852482	4089.536642	16.703155	-0.041012	3.488090
201.704096	4081.546570	16.708160	-0.040979	3.484854
201.384651	4073.604453	16.713165	-0.040915	3.481629
201.523434	4065.626714	16.718170	-0.040936	3.478401
201.533530	4057.611887	16.723175	-0.040933	3.475150
201.326083	4049.587238	16.728179	-0.040889	3.471886
201.379364	4041.569453	16.733184	-0.040894	3.468630
201.321524	4033.555767	16.738189	-0.040878	3.465368
201.317336	4025.617417	16.743194	-0.040873	3.462136
201.167917	4017.615422	16.748199	-0.040840	3.458871
201.089880	4009.616087	16.753203	-0.040820	3.455606
201.167979	4001.603370	16.758208	-0.040830	3.452337
201.001977	3993.586611	16.763213	-0.040794	3.449055
201.095212	3985.658044	16.768218	-0.040807	3.445815
201.082740	3977.609046	16.773223	-0.040799	3.442519
201.116843	3969.643927	16.778227	-0.040801	3.439256
200.858290	3961.699563	16.783232	-0.040748	3.435989
200.685824	3953.688208	16.788237	-0.040711	3.432693
200.838021	3945.658040	16.793242	-0.040734	3.429398
200.806269	3937.675655	16.798247	-0.040723	3.426113
200.948005	3929.685154	16.803251	-0.040745	3.422828
200.776414	3921.693283	16.808256	-0.040708	3.419528
200.542467	3913.728736	16.813261	-0.040659	3.416234
200.619381	3905.728845	16.818266	-0.040669	3.412932
200.531207	3897.706593	16.823271	-0.040647	3.409613
200.676263	3889.733111	16.828275	-0.040669	3.406319
200.369759	3881.761263	16.833280	-0.040607	3.403006
200.621066	3873.745402	16.838285	-0.040649	3.399692
200.786078	3865.800121	16.843290	-0.040675	3.396400
200.525349	3857.740493	16.848295	-0.040621	3.393043
200.518839	3849.687070	16.853299	-0.040615	3.389694
200.533331	3841.741048	16.858304	-0.040613	3.386387
200.446827	3833.739430	16.863309	-0.040592	3.383050
200.316402	3825.823549	16.868314	-0.040563	3.379745
199.973994	3817.862484	16.873319	-0.040494	3.376409
200.060411	3809.812435	16.878323	-0.040505	3.373048
199.914860	3801.813304	16.883328	-0.040473	3.369697
199.982401	3793.819619	16.888333	-0.040481	3.366352
200.163724	3785.821113	16.893338	-0.040510	3.363007
200.051201	3777.839381	16.898343	-0.040484	3.359654
200.057024	3769.885199	16.903347	-0.040480	3.356314
199.891585	3761.894341	16.908352	-0.040444	3.352948
199.738182	3753.855673	16.913357	-0.040411	3.349560
199.777155	3745.891498	16.918362	-0.040413	3.346207
199.879275	3737.857279	16.923367	-0.040427	3.342823
199.982956	3729.882026	16.928371	-0.040441	3.339460
199.799358	3721.948704	16.933376	-0.040402	3.336102
199.483025	3713.936950	16.938381	-0.040339	3.332702
199.714154	3705.903943	16.943386	-0.040377	3.329309
199.397146	3697.938973	16.948391	-0.040313	3.325922
199.352480	3689.986233	16.953395	-0.040299	3.322546
199.228967	3681.970674	16.958400	-0.040271	3.319138
199.282840	3674.019651	16.963405	-0.040277	3.315760
199.380508	3665.988501	16.968410	-0.040290	3.312346
199.300534	3657.951339	16.973415	-0.040270	3.308919
199.234540	3649.984230	16.978419	-0.040253	3.305519
199.099825	3642.006631	16.983424	-0.040223	3.302109
199.108470	3634.020870	16.988429	-0.040219	3.298697
199.141681	3626.048464	16.993434	-0.040221	3.295288
199.043374	3618.031980	16.998439	-0.040197	3.291851
198.903492	3610.048771	17.003443	-0.040166	3.288424
199.045233	3602.052914	17.008448	-0.040188	3.284999
198.970475	3594.097253	17.013453	-0.040169	3.281579
198.900132	3586.119047	17.018458	-0.040151	3.278145
198.925821	3578.102822	17.023463	-0.040151	3.274696
198.936287	3570.113076	17.028467	-0.040148	3.271253
198.652601	3562.107919	17.033472	-0.040090	3.267789
198.618021	3554.095135	17.038477	-0.040079	3.264328
198.876982	3546.145562	17.043482	-0.040122	3.260902
198.591647	3538.151047	17.048487	-0.040064	3.257431
198.503829	3530.176565	17.053491	-0.040043	3.253973
198.579363	3522.155980	17.058496	-0.040052	3.250498
198.499228	3514.153281	17.063501	-0.040032	3.247021
198.531461	3506.191162	17.068506	-0.040033	3.243562
198.404745	3498.199902	17.073511	-0.040004	3.240080
198.553783	3490.252575	17.078515	-0.040027	3.236625
198.502567	3482.224956	17.083520	-0.040013	3.233123
198.330395	3474.155864	17.088525	-0.039976	3.229594
198.380593	3466.210574	17.093530	-0.039980	3.226125
198.191391	3458.201360	17.098535	-0.039940	3.222614
198.107830	3450.249484	17.103539	-0.039920	3.219128
198.033269	3442.297588	17.108544	-0.039901	3.215640
197.990352	3434.286674	17.113549	-0.039888	3.212122
197.870231	3426.301083	17.118554	-0.039861	3.208609
197.899205	3418.281810	17.123559	-0.039861	3.205084
198.104727	3410.323349	17.128563	-0.039894	3.201588
197.862905	3402.385553	17.133568	-0.039844	3.198079
197.707152	3394.378387	17.138573	-0.039810	3.194540
198.036302	3386.356511	17.143578	-0.039867	3.191010
197.918850	3378.357123	17.148583	-0.039840	3.187467
197.967118	3370.360679	17.153587	-0.039844	3.183929
197.661981	3362.395060	17.158592	-0.039782	3.180386
197.914376	3354.393984	17.163597	-0.039824	3.176846
197.912062	3346.417824	17.168602	-0.039819	3.173303
197.524977	3338.395823	17.173607	-0.039742	3.169719
197.616296	3330.423697	17.178611	-0.039754	3.166174
197.710267	3322.449699	17.183616	-0.039767	3.162624
197.581959	3314.453063	17.188621	-0.039738	3.159050
197.401235	3306.521633	17.193626	-0.039699	3.155499
197.370409	3298.458322	17.198631	-0.039688	3.151891
197.354327	3290.489928	17.203635	-0.039681	3.148323
197.183407	3282.485879	17.208640	-0.039644	3.144728
197.117512	3274.550294	17.213645	-0.039627	3.141164
197.130579	3266.562511	17.218650	-0.039624	3.137576
197.047329	3258.532998	17.223655	-0.039604	3.133960
197.101863	3250.535225	17.228659	-0.039609	3.130361
197.257659	3242.554605	17.233664	-0.039633	3.126770
197.107371	3234.580224	17.238669	-0.039600	3.123164
197.080434	3226.633265	17.243674	-0.039590	3.119572
196.993750	3218.645553	17.248679	-0.039569	3.115955
197.016004	3210.637704	17.253683	-0.039568	3.112329
196.776787	3202.659096	17.258688	-0.039519	3.108700
196.894539	3194.645963	17.263693	-0.039536	3.105068
196.693230	3186.709144	17.268698	-0.039493	3.101451
196.457126	3178.713184	17.273703	-0.039444	3.097802
196.511978	3170.725568	17.278707	-0.039450	3.094165
196.732536	3162.703932	17.283712	-0.039486	3.090517
196.633988	3154.722527	17.288717	-0.039463	3.086867
196.368090	3146.766184	17.293722	-0.039408	3.083217
196.372909	3138.761957	17.298727	-0.039404	3.079554
196.414035	3130.818711	17.303731	-0.039407	3.075915
196.349362	3122.747373	17.308736	-0.039390	3.072209
196.312809	3114.725730	17.313741	-0.039378	3.068522
196.342026	3106.768081	17.318746	-0.039379	3.064863
196.137983	3098.830248	17.323751	-0.039336	3.061199
196.353266	3090.837364	17.328755	-0.039371	3.057524
196.147529	3082.874261	17.333760	-0.039328	3.053838
195.950502	3074.847746	17.338765	-0.039286	3.050119
196.005212	3066.900905	17.343770	-0.039291	3.046445
195.880931	3058.910061	17.348775	-0.039263	3.042737
195.895892	3050.919988	17.353779	-0.039261	3.039031
195.843755	3042.972143	17.358784	-0.039246	3.035337
195.737165	3034.953100	17.363789	-0.039222	3.031604
195.919605	3026.957464	17.368794	-0.039251	3.027890
195.702989	3018.985052	17.373799	-0.039205	3.024163
195.664436	3011.014672	17.378803	-0.039193	3.020441
195.883520	3003.021156	17.383808	-0.039229	3.016717
195.539991	2995.043723	17.388813	-0.039160	3.012968
195.638511	2987.038611	17.393818	-0.039174	3.009222
195.422238	2979.054599	17.398823	-0.039128	3.005467
195.511202	2971.096325	17.403827	-0.039140	3.001734
195.545710	2963.116500	17.408832	-0.039142	2.997984
195.349035	2955.139303	17.413837	-0.039100	2.994218
195.321870	2947.126471	17.418842	-0.039090	2.990440
195.087583	2939.139174	17.423847	-0.039041	2.986658
195.169155	2931.163492	17.428851	-0.039052	2.982893
195.133745	2923.170749	17.433856	-0.039040	2.979109
195.117641	2915.205215	17.438861	-0.039032	2.975334
195.006238	2907.213958	17.443866	-0.039007	2.971537
194.890681	2899.226850	17.448871	-0.038980	2.967738
195.142304	2891.225692	17.453875	-0.039022	2.963945
195.132713	2883.277812	17.458880	-0.039015	2.960160
194.954250	2875.329513	17.463885	-0.038977	2.956360
194.885895	2867.333243	17.468890	-0.038959	2.952539
194.601219	2859.337475	17.473895	-0.038902	2.948702
194.815656	2851.313177	17.478899	-0.038936	2.944872
194.811692	2843.363268	17.483904	-0.038931	2.941061
194.765183	2835.386687	17.488909	-0.038917	2.937230
194.880668	2827.392504	17.493914	-0.038934	2.933395
194.554137	2819.394057	17.498919	-0.038868	2.929529
194.737984	2811.419187	17.503923	-0.038897	2.925696
194.598844	2803.463525	17.508928	-0.038867	2.921850
194.520425	2795.487211	17.513933	-0.038847	2.917993
194.405351	2787.522933	17.518938	-0.038821	2.914134
194.051906	2779.455743	17.523943	-0.038750	2.910207
194.249927	2771.450732	17.528947	-0.038782	2.906335
194.419407	2763.494124	17.533952	-0.038808	2.902480
194.165632	2755.528120	17.538957	-0.038756	2.898592
194.003204	2747.598048	17.543962	-0.038721	2.894721
194.071362	2739.573730	17.548967	-0.038729	2.890812
193.998311	2731.590634	17.553971	-0.038710	2.886910
193.992649	2723.628087	17.558976	-0.038704	2.883016
193.820178	2715.655416	17.563981	-0.038667	2.879103
193.800882	2707.714727	17.568986	-0.038659	2.875208
193.769998	2699.697778	17.573991	-0.038648	2.871271
193.774891	2691.694808	17.578995	-0.038644	2.867336
193.740145	2683.740861	17.584000	-0.038633	2.863418
193.735200	2675.745735	17.589005	-0.038627	2.859477
193.615147	2667.815694	17.594010	-0.038600	2.855555
193.562296	2659.794988	17.599015	-0.038585	2.851587
193.656841	2651.795261	17.604019	-0.038597	2.847632
193.632544	2643.838948	17.609024	-0.038588	2.843686
193.338739	2635.872761	17.614029	-0.038528	2.839715
193.442184	2627.912854	17.619034	-0.038543	2.835764
193.295577	2619.897219	17.624039	-0.038510	2.831765
193.292089	2611.919830	17.629043	-0.038505	2.827788
193.343203	2603.926176	17.634048	-0.038509	2.823800
193.128679	2595.973580	17.639053	-0.038465	2.819812
193.151345	2588.016359	17.644058	-0.038464	2.815830
193.298236	2579.982681	17.649063	-0.038486	2.811811
193.366463	2572.006123	17.654067	-0.038494	2.807810
193.155619	2564.050110	17.659072	-0.038450	2.803798
192.958040	2556.091677	17.664077	-0.038408	2.799779
193.199244	2548.121864	17.669082	-0.038448	2.795774
193.089198	2540.109508	17.674087	-0.038423	2.791722
192.939438	2532.152937	17.679091	-0.038390	2.787690
192.902614	2524.171421	17.684096	-0.038378	2.783645
192.848169	2516.201730	17.689101	-0.038363	2.779600
192.845522	2508.253597	17.694106	-0.038358	2.775563
192.582911	2500.256015	17.699111	-0.038304	2.771479
192.666511	2492.254958	17.704115	-0.038314	2.767409
192.446016	2484.312889	17.709120	-0.038269	2.763344
192.442893	2476.317416	17.714125	-0.038263	2.759259
192.522319	2468.371023	17.719130	-0.038273	2.755198
192.344453	2460.319278	17.724135	-0.038235	2.751061
192.366260	2452.326696	17.729139	-0.038234	2.746961
192.250509	2444.368966	17.734144	-0.038207	2.742864
192.295123	2436.387237	17.739149	-0.038211	2.738758
192.492186	2428.427816	17.744154	-0.038243	2.734667
192.238229	2420.450369	17.749159	-0.038190	2.730533
192.298243	2412.473740	17.754163	-0.038197	2.726412
192.219712	2404.510581	17.759168	-0.038177	2.722283
191.961415	2396.575583	17.764173	-0.038124	2.718152
191.986787	2388.623690	17.769178	-0.038124	2.714023
191.850301	2380.613309	17.774183	-0.038094	2.709847
191.705472	2372.654670	17.779187	-0.038062	2.705692
191.652128	2364.692566	17.784192	-0.038047	2.701533
191.764409	2356.678058	17.789197	-0.038063	2.697352
191.767215	2348.721284	17.794202	-0.038058	2.693187
191.483545	2340.752477	17.799207	-0.038001	2.688991
191.599515	2332.754495	17.804211	-0.038017	2.684799
191.829353	2324.794892	17.809216	-0.038055	2.680628
191.712059	2316.839887	17.814221	-0.038028	2.676430
191.589781	2308.860779	17.819226	-0.038001	2.672213
191.506306	2300.850649	17.824231	-0.037980	2.667975
191.338408	2292.888923	17.829235	-0.037944	2.663751
191.449447	2284.911176	17.834240	-0.037960	2.659529
191.275330	2276.978531	17.839245	-0.037922	2.655307
191.208589	2268.981516	17.844250	-0.037905	2.651050
191.176551	2260.998689	17.849255	-0.037894	2.646796
190.963964	2253.065501	17.854259	-0.037850	2.642550
191.027019	2245.095810	17.859264	-0.037857	2.638295
190.996970	2237.117179	17.864269	-0.037846	2.634023
190.897830	2229.140247	17.869274	-0.037823	2.629741
190.833199	2221.161641	17.874279	-0.037806	2.625452
190.970185	2213.173472	17.879283	-0.037826	2.621165
190.795478	2205.237213	17.884288	-0.037789	2.616878
190.839452	2197.240082	17.889293	-0.037792	2.612566
190.846592	2189.268783	17.894298	-0.037788	2.608258
190.623204	2181.315155	17.899303	-0.037742	2.603937
190.642419	2173.348336	17.904307	-0.037741	2.599618
190.586330	2165.414484	17.909312	-0.037725	2.595305
190.535566	2157.242653	17.914317	-0.037711	2.590855
190.496934	2149.291114	17.919322	-0.037699	2.586518
190.472876	2141.337386	17.924327	-0.037689	2.582174
190.487179	2133.407915	17.929331	-0.037687	2.577839
190.287093	2125.488294	17.934336	-0.037645	2.573487
190.304341	2117.451038	17.939341	-0.037643	2.569078
190.451201	2109.512210	17.944346	-0.037666	2.564724
190.284327	2101.591036	17.949351	-0.037630	2.560351
190.045580	2093.669404	17.954355	-0.037580	2.555966
190.096640	2085.679862	17.959360	-0.037585	2.551555
190.025671	2077.693112	17.964365	-0.037567	2.547130
190.067178	2069.738318	17.969370	-0.037569	2.542722
190.218223	2061.730533	17.974375	-0.037593	2.538286
190.033113	2053.802256	17.979379	-0.037553	2.533862
189.928229	2045.823670	17.984384	-0.037529	2.529407
189.882899	2037.851014	17.989389	-0.037515	2.524953
190.087724	2029.904159	17.994394	-0.037549	2.520523
189.892300	2021.970199	17.999399	-0.037507	2.516064
189.877520	2013.966617	18.004403	-0.037500	2.511570
189.812306	2005.978862	18.009408	-0.037483	2.507074
189.695728	1998.021506	18.014413	-0.037456	2.502583
189.612987	1990.104805	18.019418	-0.037436	2.498110
189.437190	1982.131881	18.024423	-0.037398	2.493590
189.391832	1974.152213	18.029427	-0.037385	2.489067
189.304329	1966.192536	18.034432	-0.037363	2.484544
189.293576	1958.232489	18.039437	-0.037357	2.480019
189.291999	1950.292897	18.044442	-0.037351	2.475497
189.045073	1942.320228	18.049447	-0.037300	2.470931
188.914791	1934.359775	18.054451	-0.037271	2.466371
189.039547	1926.381600	18.059456	-0.037290	2.461812
189.059953	1918.411390	18.064461	-0.037288	2.457241
188.821611	1910.474710	18.069466	-0.037239	2.452661
188.844787	1902.472898	18.074471	-0.037239	2.448055
188.842872	1894.517532	18.079475	-0.037233	2.443465
188.741213	1886.590509	18.084480	-0.037209	2.438875
188.610697	1878.637027	18.089485	-0.037180	2.434260
188.801930	1870.561880	18.094490	-0.037211	2.429589
188.713001	1862.612948	18.099495	-0.037189	2.424961
188.482641	1854.697699	18.104499	-0.037142	2.420333
188.534976	1846.751951	18.109504	-0.037146	2.415701
188.348304	1838.783532	18.114509	-0.037107	2.411027
188.324742	1830.834002	18.119514	-0.037097	2.406368
188.302579	1822.859037	18.124519	-0.037088	2.401686
188.150390	1814.937657	18.129523	-0.037055	2.397015
188.097951	1806.989897	18.134528	-0.037040	2.392328
187.934780	1799.006256	18.139533	-0.037005	2.387601
188.056509	1791.047009	18.144538	-0.037023	2.382902
187.974657	1783.093328	18.149543	-0.037003	2.378181
188.043870	1775.119698	18.154547	-0.037011	2.373451
188.006589	1767.156321	18.159552	-0.036999	2.368709
187.875965	1759.211282	18.164557	-0.036970	2.363960
187.789522	1751.289631	18.169562	-0.036949	2.359220
187.541517	1743.363061	18.174567	-0.036898	2.354454
187.581734	1735.339097	18.179571	-0.036900	2.349643
187.545631	1727.387262	18.184576	-0.036888	2.344860
187.404505	1719.448832	18.189581	-0.036857	2.340066
187.542309	1711.484972	18.194586	-0.036878	2.335270
187.492401	1703.510323	18.199591	-0.036864	2.330443
187.263484	1695.586905	18.204595	-0.036816	2.325621
187.412919	1687.616106	18.209600	-0.036839	2.320792
187.391583	1679.674362	18.214605	-0.036830	2.315956
187.394032	1671.714762	18.219610	-0.036826	2.311101
187.184621	1663.761109	18.224615	-0.036782	2.306222
187.168953	1655.820485	18.229619	-0.036774	2.301357
187.140756	1647.877795	18.234624	-0.036764	2.296479
186.949700	1639.926997	18.239629	-0.036723	2.291572
187.086671	1631.958004	18.244634	-0.036744	2.286671
186.960582	1624.015790	18.249639	-0.036716	2.281754
186.797194	1616.094161	18.254643	-0.036680	2.276836
186.775460	1608.093997	18.259648	-0.036671	2.271870
186.703462	1600.105754	18.264653	-0.036653	2.266897
186.713185	1592.175028	18.269658	-0.036650	2.261955
186.503438	1584.238683	18.274663	-0.036606	2.256980
186.612792	1576.263356	18.279667	-0.036621	2.251998
186.513620	1568.321971	18.284672	-0.036598	2.247007
186.547710	1560.367782	18.289677	-0.036599	2.242009
186.549295	1552.445485	18.294682	-0.036595	2.237017
186.423194	1544.503170	18.299687	-0.036566	2.231990
186.502398	1536.530349	18.304691	-0.036576	2.226951
186.257465	1528.624668	18.309696	-0.036526	2.221913
186.167000	1520.680303	18.314701	-0.036504	2.216854
186.311385	1512.726465	18.319706	-0.036526	2.211798
186.270992	1504.761562	18.324711	-0.036514	2.206706
186.117299	1496.846866	18.329715	-0.036480	2.201625
185.952667	1488.932642	18.334720	-0.036445	2.196531
185.848763	1480.947084	18.339725	-0.036420	2.191385
185.950773	1472.974146	18.344730	-0.036434	2.186254
185.922087	1465.040304	18.349735	-0.036424	2.181124
185.914349	1457.098327	18.354739	-0.036418	2.175979
185.790475	1449.163546	18.359744	-0.036390	2.170815
185.823032	1441.201962	18.364749	-0.036391	2.165636
185.542285	1433.322461	18.369754	-0.036334	2.160469
185.479557	1425.387951	18.374759	-0.036317	2.155274
185.401258	1417.429878	18.379763	-0.036298	2.150050
185.497260	1409.463145	18.384768	-0.036311	2.144823
185.228130	1401.539219	18.389773	-0.036256	2.139578
185.253425	1393.612937	18.394778	-0.036255	2.134346
185.423900	1385.630077	18.399783	-0.036282	2.129077
185.288143	1377.714436	18.404787	-0.036252	2.123811
185.304954	1369.802141	18.409792	-0.036250	2.118548
185.189850	1361.842964	18.414797	-0.036224	2.113228
185.010785	1353.875367	18.419802	-0.036186	2.107883
184.837723	1345.955829	18.424807	-0.036149	2.102557
184.720588	1338.034210	18.429811	-0.036122	2.097222
184.613296	1330.107093	18.434816	-0.036097	2.091870
184.730961	1322.130020	18.439821	-0.036114	2.086493
184.752742	1314.219804	18.444826	-0.036113	2.081138
184.749052	1306.281504	18.449831	-0.036108	2.075747
184.637768	1298.360951	18.454835	-0.036082	2.070344
184.418098	1290.456640	18.459840	-0.036036	2.064927
184.552390	1282.485686	18.464845	-0.036056	2.059485
184.526561	1274.588882	18.469850	-0.036047	2.054064
184.196550	1266.667798	18.474855	-0.035980	2.048581
184.293581	1258.721495	18.479859	-0.035993	2.043109
184.409785	1250.795139	18.484864	-0.036010	2.037638
184.179192	1242.878972	18.489869	-0.035962	2.032124
184.088075	1234.937662	18.494874	-0.035940	2.026592
184.091731	1226.992470	18.499879	-0.035936	2.021052
184.105577	1219.073994	18.504883	-0.035934	2.015516
183.910314	1211.168607	18.509888	-0.035893	2.009953
183.691062	1203.245784	18.514893	-0.035847	2.004359
183.620090	1195.353513	18.519898	-0.035829	1.998786
183.613746	1187.417466	18.524903	-0.035823	1.993174
183.546376	1179.484249	18.529907	-0.035805	1.987541
183.467042	1171.574669	18.534912	-0.035786	1.981908
183.282558	1163.665916	18.539917	-0.035746	1.976249
183.445191	1155.704354	18.544922	-0.035772	1.970572
183.330909	1147.787197	18.549927	-0.035746	1.964881
183.322141	1139.888728	18.554931	-0.035739	1.959198
183.243266	1131.978938	18.559936	-0.035720	1.953483
183.050651	1124.016986	18.564941	-0.035679	1.947701
183.181985	1116.090475	18.569946	-0.035698	1.941963
183.092764	1108.172683	18.574951	-0.035677	1.936190
182.938409	1100.263808	18.579955	-0.035643	1.930400
182.998142	1092.337527	18.584960	-0.035649	1.924602
182.612148	1084.486449	18.589965	-0.035573	1.918793
182.728203	1076.553896	18.594970	-0.035589	1.912962
182.614127	1068.634052	18.599975	-0.035563	1.907097
182.562678	1060.721780	18.604979	-0.035549	1.901226
182.590001	1052.811306	18.609984	-0.035549	1.895348
182.205892	1044.926833	18.614989	-0.035473	1.889424
182.653090	1036.958161	18.619994	-0.035551	1.883512
182.571319	1029.074957	18.624999	-0.035531	1.877586
182.598546	1021.143123	18.630003	-0.035531	1.871617
182.431076	1013.246464	18.635008	-0.035495	1.865633
182.219109	1005.367862	18.640013	-0.035451	1.859639
182.334072	997.459212	18.645018	-0.035467	1.853640
182.253131	989.548439	18.650023	-0.035447	1.847597
182.137835	981.662743	18.655027	-0.035421	1.841549
182.006906	973.797498	18.660032	-0.035392	1.835496
181.844661	965.882372	18.665037	-0.035357	1.829380
181.968982	957.964582	18.670042	-0.035375	1.823275
182.152976	950.037825	18.675047	-0.035404	1.817150
181.823709	942.177010	18.680051	-0.035338	1.810995
181.869096	934.277649	18.685056	-0.035342	1.804833
181.660777	926.423777	18.690061	-0.035298	1.798655
181.461593	918.527033	18.695066	-0.035256	1.792423
181.461652	910.561775	18.700071	-0.035251	1.786139
181.512649	902.668742	18.705075	-0.035256	1.779897
181.424157	894.804808	18.710080	-0.035234	1.773639
181.326171	886.894700	18.715085	-0.035211	1.767320
181.165458	879.050945	18.720090	-0.035177	1.761025
181.111666	871.171683	18.725095	-0.035162	1.754691
181.210639	863.250579	18.730099	-0.035175	1.748320
181.049024	855.387444	18.735104	-0.035140	1.741940
180.855282	847.526781	18.740109	-0.035099	1.735534
180.968208	839.623624	18.745114	-0.035115	1.729108
180.794431	831.762155	18.750119	-0.035078	1.722656
180.860734	823.875021	18.755123	-0.035086	1.716190
180.709142	816.000011	18.760128	-0.035053	1.709681
180.681929	808.101943	18.765133	-0.035043	1.703144
180.763082	800.231126	18.770138	-0.035053	1.696619
180.526608	792.367028	18.775143	-0.035004	1.690032
180.363175	784.521830	18.780147	-0.034969	1.683445
180.433362	776.643903	18.785152	-0.034977	1.676836
180.656462	768.723145	18.790157	-0.035014	1.670185
180.451191	760.903904	18.795162	-0.034971	1.663536
180.256917	753.056607	18.800167	-0.034930	1.656837
180.321014	745.167012	18.805171	-0.034937	1.650111
180.339765	737.306690	18.810176	-0.034935	1.643375
180.106186	729.495253	18.815181	-0.034887	1.636620
180.189269	721.563093	18.820186	-0.034898	1.629776
180.032725	713.703151	18.825191	-0.034864	1.622932
179.830651	705.883751	18.830195	-0.034821	1.616088
179.711840	698.040488	18.835200	-0.034794	1.609206
179.774457	690.154927	18.840205	-0.034801	1.602283
179.591168	682.353773	18.845210	-0.034762	1.595369
179.440546	674.508760	18.850215	-0.034729	1.588391
179.546047	666.623639	18.855219	-0.034744	1.581383
179.533410	658.801388	18.860224	-0.034737	1.574383
179.232227	650.978485	18.865229	-0.034676	1.567309
179.280344	643.133464	18.870234	-0.034680	1.560234
179.209943	635.306495	18.875239	-0.034662	1.553126
179.011547	627.465665	18.880243	-0.034620	1.545954
179.003100	619.640067	18.885248	-0.034614	1.538791
178.904760	611.801420	18.890253	-0.034591	1.531568
179.008866	603.955721	18.895258	-0.034605	1.524335
178.608264	596.195178	18.900263	-0.034526	1.517070
178.674658	588.334449	18.905267	-0.034533	1.509748
178.875964	580.480194	18.910272	-0.034566	1.502417
178.629412	572.699926	18.915277	-0.034515	1.495051
178.730110	564.858623	18.920282	-0.034529	1.487644
178.449252	557.089343	18.925287	-0.034472	1.480209
178.487723	549.253561	18.930291	-0.034474	1.472723
178.258118	541.436832	18.935296	-0.034427	1.465175
178.058767	533.658971	18.940301	-0.034385	1.457630
178.044125	525.844470	18.945306	-0.034377	1.450040
178.003872	518.041679	18.950311	-0.034365	1.442417
178.013757	510.244361	18.955315	-0.034362	1.434767
177.814403	502.471131	18.960320	-0.034320	1.427066
177.735421	494.681653	18.965325	-0.034301	1.419326
177.842902	486.878662	18.970330	-0.034316	1.411561
177.814554	479.091489	18.975335	-0.034306	1.403747
177.558888	471.359050	18.980339	-0.034253	1.395906
177.502143	463.563877	18.985344	-0.034238	1.387990
177.277239	455.807497	18.990349	-0.034191	1.380041
177.315349	448.029908	18.995354	-0.034194	1.372068
176.895851	440.312642	19.000359	-0.034111	1.364032
177.026182	432.518995	19.005363	-0.034130	1.355964
177.168557	424.727672	19.010368	-0.034152	1.347853
176.846662	417.014078	19.015373	-0.034087	1.339692
176.642709	409.293372	19.020378	-0.034044	1.331495
176.627991	401.530559	19.025383	-0.034037	1.323236
176.688416	393.762109	19.030387	-0.034043	1.314933
176.512676	385.926265	19.035392	-0.034006	1.306461
176.531699	378.190401	19.040397	-0.034005	1.298078
176.538516	370.464874	19.045402	-0.034001	1.289649
176.402229	362.760657	19.050407	-0.033971	1.281162
176.348005	355.057163	19.055411	-0.033956	1.272635
176.277493	347.351839	19.060416	-0.033938	1.264045
175.922453	339.698881	19.065421	-0.033867	1.255401
176.050185	331.970845	19.070426	-0.033886	1.246704
175.999156	324.290077	19.075431	-0.033872	1.237966
175.666034	316.625302	19.080435	-0.033805	1.229128
175.483055	308.956552	19.085440	-0.033767	1.220252
175.244609	301.292979	19.090445	-0.033718	1.211306
175.435478	293.580181	19.095450	-0.033748	1.202320
175.357575	285.924172	19.100455	-0.033729	1.193281
175.113987	278.285136	19.105459	-0.033679	1.184158
175.113963	270.631605	19.110464	-0.033674	1.174998
174.825617	263.010871	19.115469	-0.033616	1.165745
174.807942	255.381570	19.120474	-0.033608	1.156464
174.701041	247.713413	19.125479	-0.033583	1.147042
174.588224	240.092472	19.130483	-0.033558	1.137599
174.533833	232.470644	19.135488	-0.033543	1.128088
174.407324	224.876826	19.140493	-0.033515	1.118516
174.474282	217.262884	19.145498	-0.033522	1.108878
174.289250	209.694362	19.150503	-0.033483	1.099158
174.033452	202.141735	19.155507	-0.033431	1.089356
174.105319	194.554714	19.160512	-0.033440	1.079494
173.828963	187.015231	19.165517	-0.033384	1.069524
173.564696	179.490806	19.170522	-0.033330	1.059483
173.459543	171.948164	19.175527	-0.033305	1.049359
173.411054	164.410329	19.180531	-0.033292	1.039156
173.247461	156.913777	19.185536	-0.033257	1.028881
173.045324	149.419317	19.190541	-0.033214	1.018495
172.955423	141.924144	19.195546	-0.033193	1.008029
173.004382	134.426354	19.200551	-0.033198	0.997484
172.815775	126.935882	19.205555	-0.033158	0.986777
172.588434	119.509203	19.210560	-0.033111	0.976035
172.588800	112.036239	19.215565	-0.033106	0.965164
172.458689	104.629373	19.220570	-0.033078	0.954233
172.118525	97.258621	19.225575	-0.033010	0.943174
171.989189	89.862739	19.230579	-0.032981	0.932002
171.804994	82.507816	19.235584	-0.032942	0.920742
171.502158	75.164592	19.240589	-0.032881	0.909328
171.287132	67.838168	19.245594	-0.032837	0.897820
170.914554	60.772553	19.250599	-0.032763	0.886534