Thu Mar 11 18:53:15 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.687291	-0.013201	0.000000	0.000003	0.725122

0.650861	-0.122489	0.005005	0.000010	0.724896
0.566853	-0.113214	0.010010	0.000025	0.724886
0.792794	-0.150461	0.015014	-0.000017	0.724892
0.765496	-0.148768	0.020019	-0.000012	0.724886
0.716797	-0.140673	0.025024	-0.000004	0.724886
0.671167	-0.131447	0.030029	0.000005	0.724888
0.789768	-0.156168	0.035034	-0.000018	0.724882
0.797363	-0.152788	0.040038	-0.000019	0.724892
0.654052	-0.131200	0.045043	0.000007	0.724884
0.661423	-0.131171	0.050048	0.000005	0.724887
0.683192	-0.134463	0.055053	0.000001	0.724889
0.540193	-0.113410	0.060058	0.000027	0.724881
0.645383	-0.126486	0.065062	0.000008	0.724893
0.677905	-0.138595	0.070067	0.000001	0.724881
0.720868	-0.156831	0.075072	-0.000007	0.724860
0.734831	-0.295110	0.080077	-0.000010	0.724595
0.756916	-0.303563	0.085082	-0.000014	0.724587
0.819772	-0.310941	0.090086	-0.000026	0.724595
0.897834	-0.327964	0.095091	-0.000041	0.724589
0.831187	-0.315317	0.100096	-0.000029	0.724591
0.562256	-0.265221	0.105101	0.000021	0.724596
0.715062	-0.429245	0.110106	-0.000008	0.724329
0.615656	-0.445407	0.115110	0.000011	0.724263
0.689503	-0.461400	0.120115	-0.000003	0.724258
0.381400	-0.406882	0.125120	0.000054	0.724258
0.541769	-0.432818	0.130125	0.000024	0.724263
0.540780	-0.531980	0.135130	0.000024	0.724069
0.689061	-0.616812	0.140134	-0.000004	0.723955
0.759885	-0.631788	0.145139	-0.000018	0.723951
0.842266	-0.644996	0.150144	-0.000033	0.723955
0.801386	-0.709289	0.155149	-0.000026	0.723815
0.803846	-0.803946	0.160154	-0.000027	0.723631
1.164050	-0.863792	0.165158	-0.000094	0.723640
0.814460	-0.804195	0.170163	-0.000029	0.723635
0.686168	-0.920699	0.175168	-0.000005	0.723362
0.582003	-0.911246	0.180173	0.000014	0.723345
0.472938	-0.895904	0.185178	0.000034	0.723338
0.702822	-1.022195	0.190182	-0.000009	0.723171
0.590188	-1.087561	0.195187	0.000012	0.723004
0.806954	-1.126093	0.200192	-0.000029	0.723004
0.774566	-1.190649	0.205197	-0.000023	0.722867
0.658838	-1.261793	0.210202	-0.000002	0.722687
0.723010	-1.268939	0.215206	-0.000014	0.722696
0.530958	-1.333947	0.220211	0.000021	0.722502
0.474585	-1.391678	0.225216	0.000032	0.722370
0.500125	-1.395527	0.230221	0.000027	0.722371
0.507718	-1.521474	0.235226	0.000025	0.722127
0.548822	-1.553927	0.240230	0.000017	0.722078
0.347738	-1.549572	0.245235	0.000054	0.722017
0.268335	-1.675182	0.250240	0.000069	0.721743
0.348237	-1.687520	0.255245	0.000054	0.721747
0.347351	-1.789095	0.260250	0.000054	0.721548
0.340304	-1.840670	0.265254	0.000055	0.721445
0.424295	-1.891814	0.270259	0.000039	0.721374
0.462101	-2.027058	0.275264	0.000032	0.721122
0.522946	-2.034496	0.280269	0.000020	0.721129
0.586935	-2.169003	0.285274	0.000008	0.720887
0.294591	-2.117755	0.290278	0.000062	0.720886
-0.023458	-2.192239	0.295283	0.000121	0.720629
0.221000	-2.280563	0.300288	0.000076	0.720541
-0.057359	-2.313724	0.305293	0.000127	0.720379
-0.481011	-2.317740	0.310298	0.000206	0.720223
-0.258008	-2.399049	0.315302	0.000164	0.720141
-3.242455	-1.990577	0.320307	0.000719	0.719900
-3.132556	-2.010364	0.325312	0.000698	0.719900
-3.627694	-1.919945	0.330317	0.000790	0.719905
-3.711619	-2.038226	0.335322	0.000806	0.719643
-4.276629	-1.954768	0.340326	0.000911	0.719609
-4.852969	-1.856579	0.345331	0.001018	0.719601
-4.635399	-1.894948	0.350336	0.000977	0.719602
-4.452578	-2.013487	0.355341	0.000943	0.719433
-5.952000	-1.831060	0.360346	0.001221	0.719267
-5.345610	-1.935115	0.365350	0.001108	0.719275
-5.433118	-1.924099	0.370355	0.001124	0.719267
-5.588686	-1.894550	0.375360	0.001153	0.719271
-5.368114	-2.036194	0.380365	0.001112	0.719069
-6.880893	-1.825266	0.385370	0.001393	0.718955
-6.319495	-1.920797	0.390374	0.001288	0.718964
-6.039282	-1.973807	0.395379	0.001236	0.718958
-6.756827	-1.845990	0.400384	0.001369	0.718959
-6.470570	-1.934257	0.405389	0.001316	0.718886
-7.270374	-1.917721	0.410394	0.001464	0.718638
-7.325737	-1.902223	0.415398	0.001474	0.718649
-7.612873	-1.854700	0.420403	0.001528	0.718643
-7.207832	-1.926343	0.425408	0.001452	0.718644
-7.042388	-1.953968	0.430413	0.001421	0.718648
-7.798678	-1.867964	0.435418	0.001561	0.718553
-8.242002	-1.886751	0.440422	0.001644	0.718360
-7.875067	-1.955522	0.445427	0.001575	0.718354
-8.574500	-1.832230	0.450432	0.001705	0.718352
-8.208137	-1.894575	0.455437	0.001637	0.718358
-8.214544	-1.896930	0.460442	0.001637	0.718352
-8.138071	-1.929739	0.465446	0.001623	0.718314
-8.986742	-1.929992	0.470451	0.001781	0.718016
-8.894306	-1.946394	0.475456	0.001763	0.718017
-9.318671	-1.867667	0.480461	0.001842	0.718023
-9.334967	-1.870314	0.485466	0.001845	0.718013
-8.758610	-1.968563	0.490470	0.001737	0.718022
-9.137344	-1.903533	0.495475	0.001807	0.718018
-9.632801	-1.932507	0.500480	0.001899	0.717787
-10.029615	-1.901459	0.505485	0.001973	0.717709
-9.943977	-1.920798	0.510490	0.001957	0.717701
-9.907107	-1.923355	0.515494	0.001950	0.717710
-10.461633	-1.828196	0.520499	0.002053	0.717703
-10.452539	-1.829084	0.525504	0.002051	0.717705
-9.582044	-1.980557	0.530509	0.001888	0.717712
-10.670327	-1.937360	0.535514	0.002091	0.717415
-11.301764	-1.839512	0.540518	0.002208	0.717387
-11.044003	-1.886982	0.545523	0.002160	0.717384
-10.843652	-1.924305	0.550528	0.002122	0.717381
-10.826275	-1.925366	0.555533	0.002119	0.717386
-11.063123	-1.887578	0.560538	0.002163	0.717378
-10.977682	-1.900052	0.565542	0.002146	0.717384
-11.457840	-1.937202	0.570547	0.002236	0.717142
-11.907564	-1.887456	0.575552	0.002319	0.717082
-11.628190	-1.934830	0.580557	0.002267	0.717087
-12.094477	-1.855619	0.585562	0.002353	0.717080
-12.028284	-1.863009	0.590566	0.002341	0.717089
-11.736428	-1.917223	0.595571	0.002286	0.717086
-12.306904	-1.815034	0.600576	0.002392	0.717087
-12.304067	-1.923766	0.605581	0.002391	0.716874
-13.139143	-1.836560	0.610586	0.002546	0.716752
-12.747001	-1.902762	0.615590	0.002473	0.716760
-13.073460	-1.847941	0.620595	0.002534	0.716754
-13.231574	-1.820623	0.625600	0.002563	0.716753
-12.580796	-1.932580	0.630605	0.002441	0.716761
-13.113288	-1.842558	0.635610	0.002540	0.716752
-13.367161	-1.792504	0.640614	0.002587	0.716762
-13.330695	-1.951958	0.645619	0.002580	0.716460
-13.666578	-1.900383	0.650624	0.002642	0.716444
-13.904989	-1.854622	0.655629	0.002687	0.716451
-13.705764	-1.893873	0.660634	0.002649	0.716444
-13.751601	-1.880839	0.665638	0.002658	0.716454
-14.003950	-1.839572	0.670643	0.002704	0.716447
-14.010198	-1.839581	0.675648	0.002705	0.716446
-13.825294	-1.992978	0.680653	0.002670	0.716208
-15.110248	-1.805591	0.685658	0.002909	0.716126
-14.830729	-1.851305	0.690662	0.002857	0.716134
-14.330503	-1.942480	0.695667	0.002764	0.716131
-14.709709	-1.874791	0.700672	0.002834	0.716132
-14.654515	-1.879598	0.705677	0.002823	0.716142
-14.738088	-1.870088	0.710682	0.002839	0.716132
-14.541618	-1.994177	0.715686	0.002802	0.715956
-15.513996	-1.857530	0.720691	0.002983	0.715884
-15.761222	-1.814729	0.725696	0.003028	0.715882
-14.966655	-1.953652	0.730701	0.002880	0.715888
-15.389570	-1.883020	0.735706	0.002959	0.715879
-15.654923	-1.831516	0.740710	0.003008	0.715888
-15.412635	-1.888322	0.745715	0.002963	0.715861
-15.968955	-1.949692	0.750720	0.003066	0.715544
-16.268168	-1.893062	0.755725	0.003121	0.715551
-16.720643	-1.816058	0.760730	0.003205	0.715544
-16.345245	-1.879369	0.765734	0.003135	0.715552
-16.359625	-1.880212	0.770739	0.003138	0.715546
-16.676078	-1.823266	0.775744	0.003196	0.715547
-16.217828	-1.902478	0.780749	0.003111	0.715552
-16.926161	-1.940234	0.785754	0.003242	0.715228
-17.634412	-1.810618	0.790758	0.003374	0.715235
-17.427171	-1.849642	0.795763	0.003335	0.715232
-17.218665	-1.888064	0.800768	0.003296	0.715229
-17.650311	-1.808668	0.805773	0.003376	0.715235
-17.673000	-1.808265	0.810778	0.003380	0.715228
-17.168324	-1.893981	0.815782	0.003286	0.715237
-17.374277	-1.944101	0.820787	0.003324	0.715065
-18.962372	-1.741559	0.825792	0.003619	0.714906
-18.065117	-1.899262	0.830797	0.003452	0.714911
-18.142083	-1.889306	0.835802	0.003466	0.714904
-18.526119	-1.817880	0.840806	0.003537	0.714911
-18.119435	-1.892946	0.845811	0.003461	0.714906
-18.050264	-1.906350	0.850816	0.003448	0.714904
-18.234116	-1.914240	0.855821	0.003482	0.714824
-19.569082	-1.786993	0.860826	0.003730	0.714605
-19.084405	-1.868720	0.865830	0.003640	0.714615
-19.184420	-1.853870	0.870835	0.003658	0.714609
-19.360709	-1.822915	0.875840	0.003691	0.714609
-19.106432	-1.868588	0.880845	0.003643	0.714609
-19.382903	-1.822576	0.885850	0.003694	0.714603
-19.523781	-1.791797	0.890854	0.003720	0.714615
-19.122742	-1.966404	0.895859	0.003645	0.714410
-20.234622	-1.836316	0.900864	0.003852	0.714276
-20.090466	-1.858875	0.905869	0.003825	0.714283
-20.475160	-1.795779	0.910874	0.003896	0.714272
-20.189592	-1.842471	0.915878	0.003843	0.714281
-20.059927	-1.867556	0.920883	0.003819	0.714278
-20.536858	-1.783391	0.925888	0.003907	0.714276
-20.355042	-1.833916	0.930893	0.003873	0.714241
-20.787372	-1.895069	0.935898	0.003953	0.713967
-21.090896	-1.838105	0.940902	0.004009	0.713973
-21.663024	-1.736507	0.945907	0.004116	0.713973
-21.253258	-1.810591	0.950912	0.004039	0.713971
-21.143112	-1.829017	0.955917	0.004018	0.713974
-21.699687	-1.735099	0.960922	0.004122	0.713964
-21.169531	-1.826588	0.965926	0.004023	0.713971
-20.959130	-1.924650	0.970931	0.003983	0.713851
-22.126424	-1.818780	0.975936	0.004200	0.713648
-21.622597	-1.903932	0.980941	0.004106	0.713658
-22.084237	-1.828259	0.985946	0.004192	0.713646
-22.289548	-1.789697	0.990950	0.004230	0.713650
-21.962881	-1.849527	0.995955	0.004169	0.713647
-21.979385	-1.846998	1.000960	0.004172	0.713647
-22.129272	-1.860234	1.005965	0.004199	0.713568
-23.361170	-1.748849	1.010970	0.004428	0.713354
-22.635074	-1.875138	1.015974	0.004293	0.713360
-22.806268	-1.844813	1.020979	0.004325	0.713360
-23.150673	-1.785510	1.025984	0.004388	0.713357
-22.858834	-1.834074	1.030989	0.004334	0.713364
-22.688750	-1.867929	1.035994	0.004302	0.713358
-22.743983	-1.891303	1.040998	0.004312	0.713292
-23.959179	-1.809909	1.046003	0.004538	0.713024
-23.912714	-1.820012	1.051008	0.004529	0.713021
-23.570127	-1.877463	1.056013	0.004465	0.713028
-23.736699	-1.852315	1.061018	0.004496	0.713020
-23.918846	-1.816860	1.066022	0.004529	0.713026
-23.835645	-1.834175	1.071027	0.004514	0.713022
-23.723971	-1.854759	1.076032	0.004492	0.713021
-24.247085	-1.904736	1.081037	0.004590	0.712736
-24.728307	-1.835203	1.086042	0.004679	0.712705
-24.541977	-1.866424	1.091046	0.004644	0.712709
-24.515390	-1.871691	1.096051	0.004639	0.712708
-24.781405	-1.824861	1.101056	0.004688	0.712708
-24.719079	-1.833320	1.106061	0.004676	0.712714
-24.983295	-1.791594	1.111066	0.004725	0.712703
-25.069444	-1.903215	1.116070	0.004741	0.712451
-25.328445	-1.890590	1.121075	0.004789	0.712385
-25.620085	-1.839271	1.126080	0.004843	0.712384
-25.569476	-1.843920	1.131085	0.004833	0.712393
-25.537737	-1.855238	1.136090	0.004827	0.712383
-25.391502	-1.878258	1.141094	0.004800	0.712389
-25.826022	-1.801246	1.146099	0.004880	0.712389
-26.325470	-1.834151	1.151104	0.004973	0.712146
-26.294482	-1.864800	1.156109	0.004967	0.712097
-26.375776	-1.855112	1.161114	0.004982	0.712088
-26.284761	-1.867903	1.166118	0.004965	0.712095
-26.292914	-1.868390	1.171123	0.004966	0.712092
-26.418508	-1.847871	1.176128	0.004989	0.712089
-26.312305	-1.863486	1.181133	0.004969	0.712096
-26.919550	-1.907276	1.186138	0.005082	0.711793
-27.388250	-1.836698	1.191142	0.005169	0.711768
-27.370247	-1.843567	1.196147	0.005165	0.711761
-27.122611	-1.889357	1.201152	0.005119	0.711758
-27.040145	-1.900666	1.206157	0.005103	0.711766
-27.598113	-1.806429	1.211162	0.005207	0.711756
-27.507790	-1.818708	1.216166	0.005190	0.711764
-27.429891	-1.951168	1.221171	0.005175	0.711528
-28.376903	-1.820825	1.226176	0.005351	0.711452
-28.502079	-1.795409	1.231181	0.005374	0.711459
-28.343070	-1.828616	1.236186	0.005344	0.711449
-28.135980	-1.862095	1.241190	0.005305	0.711457
-28.301228	-1.833295	1.246195	0.005336	0.711456
-28.596078	-1.783396	1.251200	0.005390	0.711451
-28.064171	-1.947805	1.256205	0.005291	0.711313
-29.190491	-1.837244	1.261210	0.005500	0.711133
-29.047181	-1.861081	1.266214	0.005474	0.711137
-29.008923	-1.869952	1.271219	0.005466	0.711134
-29.212168	-1.834068	1.276224	0.005504	0.711134
-28.943686	-1.878646	1.281229	0.005453	0.711141
-29.242872	-1.829693	1.286234	0.005509	0.711132
-29.230158	-1.903076	1.291238	0.005506	0.710991
-29.971839	-1.831807	1.296243	0.005644	0.710870
-29.962525	-1.835755	1.301248	0.005642	0.710866
-29.475300	-1.917634	1.306253	0.005551	0.710876
-29.855910	-1.855811	1.311258	0.005622	0.710865
-30.054492	-1.817004	1.316262	0.005658	0.710872
-29.508991	-1.915015	1.321267	0.005557	0.710871
-30.219199	-1.943692	1.326272	0.005689	0.710562
-30.842734	-1.845999	1.331277	0.005804	0.710535
-31.170155	-1.791618	1.336282	0.005865	0.710528
-30.699759	-1.872652	1.341286	0.005777	0.710534
-30.714360	-1.872103	1.346291	0.005780	0.710530
-31.321557	-1.767825	1.351296	0.005892	0.710523
-30.663330	-1.880026	1.356301	0.005770	0.710534
-30.893256	-1.958980	1.361306	0.005812	0.710295
-31.767470	-1.843362	1.366310	0.005975	0.710215
-31.592033	-1.874218	1.371315	0.005942	0.710216
-31.678242	-1.861062	1.376320	0.005958	0.710212
-31.648243	-1.863383	1.381325	0.005952	0.710219
-31.737528	-1.850968	1.386330	0.005968	0.710212
-31.621915	-1.868819	1.391334	0.005946	0.710218
-32.156801	-1.918824	1.396339	0.006046	0.709928
-33.001812	-1.787031	1.401344	0.006203	0.709891
-32.396944	-1.893091	1.406349	0.006090	0.709895
-32.291642	-1.915782	1.411354	0.006070	0.709888
-32.667801	-1.847361	1.416358	0.006140	0.709891
-32.700353	-1.841620	1.421363	0.006145	0.709892
-32.490733	-1.881262	1.426368	0.006106	0.709888
-32.660502	-1.969064	1.431373	0.006138	0.709652
-33.839516	-1.789169	1.436378	0.006357	0.709592
-33.522569	-1.843373	1.441382	0.006298	0.709597
-33.266719	-1.892191	1.446387	0.006250	0.709591
-33.896754	-1.780397	1.451392	0.006367	0.709591
-33.559542	-1.835871	1.456397	0.006304	0.709601
-33.180768	-1.908391	1.461402	0.006233	0.709591
-33.784140	-1.917148	1.466406	0.006345	0.709359
-34.570584	-1.824831	1.471411	0.006491	0.709264
-34.426199	-1.853744	1.476416	0.006464	0.709258
-33.909815	-1.941154	1.481421	0.006368	0.709268
-34.632265	-1.817216	1.486426	0.006502	0.709258
-34.444297	-1.847578	1.491430	0.006466	0.709265
-34.240340	-1.885977	1.496435	0.006428	0.709262
-34.955697	-1.835918	1.501440	0.006561	0.709107
-35.469397	-1.817220	1.506445	0.006657	0.708962
-35.247936	-1.860375	1.511450	0.006615	0.708955
-35.338665	-1.842316	1.516454	0.006632	0.708959
-35.367598	-1.838623	1.521459	0.006637	0.708957
-35.157405	-1.878991	1.526464	0.006597	0.708952
-34.890450	-1.921171	1.531469	0.006547	0.708963
-35.656659	-1.831532	1.536474	0.006690	0.708869
-36.034870	-1.876703	1.541478	0.006760	0.708644
-35.677199	-1.940901	1.546483	0.006693	0.708644
-36.609754	-1.778259	1.551488	0.006866	0.708637
-36.240703	-1.841563	1.556493	0.006798	0.708643
-35.855736	-1.916002	1.561498	0.006726	0.708632
-36.202616	-1.852173	1.566502	0.006790	0.708636
-36.275787	-1.880651	1.571507	0.006803	0.708554
-37.191194	-1.821260	1.576512	0.006973	0.708346
-36.775238	-1.893004	1.581517	0.006896	0.708352
-37.042303	-1.850216	1.586522	0.006945	0.708342
-37.148855	-1.829377	1.591526	0.006965	0.708347
-36.808510	-1.890098	1.596531	0.006901	0.708347
-37.183188	-1.824819	1.601536	0.006971	0.708345
-37.101624	-1.867499	1.606541	0.006955	0.708289
-37.972899	-1.855409	1.611546	0.007117	0.708002
-37.902723	-1.862021	1.616550	0.007104	0.708014
-38.139602	-1.821807	1.621555	0.007148	0.708011
-38.049265	-1.842018	1.626560	0.007131	0.708003
-37.836424	-1.876277	1.631565	0.007091	0.708011
-38.307314	-1.795522	1.636570	0.007178	0.708005
-38.033713	-1.841195	1.641574	0.007127	0.708012
-37.912840	-1.979730	1.646579	0.007104	0.707778
-39.285159	-1.777295	1.651584	0.007359	0.707694
-38.964318	-1.829600	1.656589	0.007299	0.707704
-38.764720	-1.870569	1.661594	0.007262	0.707694
-38.934187	-1.838789	1.666598	0.007293	0.707698
-38.783307	-1.864497	1.671603	0.007265	0.707700
-39.159690	-1.802296	1.676608	0.007335	0.707691
-39.060703	-1.909878	1.681613	0.007316	0.707511
-39.936983	-1.824309	1.686618	0.007479	0.707370
-39.915885	-1.826652	1.691622	0.007475	0.707373
-39.787606	-1.849772	1.696627	0.007450	0.707373
-39.983323	-1.816347	1.701632	0.007487	0.707371
-39.690799	-1.865826	1.706637	0.007432	0.707377
-39.886260	-1.835598	1.711642	0.007468	0.707368
-40.011528	-1.856889	1.716646	0.007491	0.707281
-40.739906	-1.827321	1.721651	0.007626	0.707080
-40.436897	-1.884037	1.726656	0.007570	0.707075
-40.548938	-1.858761	1.731661	0.007590	0.707087
-40.922893	-1.796986	1.736666	0.007660	0.707077
-40.844737	-1.808256	1.741670	0.007645	0.707083
-40.453263	-1.878835	1.746675	0.007572	0.707082
-40.622294	-1.882783	1.751680	0.007603	0.707014
-41.458244	-1.863261	1.756685	0.007758	0.706755
-41.432491	-1.870671	1.761690	0.007753	0.706749
-41.610427	-1.836955	1.766694	0.007786	0.706754
-41.396912	-1.875853	1.771699	0.007746	0.706753
-41.798931	-1.807827	1.776704	0.007821	0.706746
-41.507432	-1.856390	1.781709	0.007766	0.706753
-41.505126	-1.878312	1.786714	0.007766	0.706711
-42.409907	-1.849566	1.791718	0.007934	0.706445
-42.274906	-1.874119	1.796723	0.007908	0.706444
-42.673878	-1.804692	1.801728	0.007982	0.706442
-42.174833	-1.891730	1.806733	0.007889	0.706446
-42.133663	-1.902587	1.811738	0.007881	0.706439
-42.590857	-1.820334	1.816742	0.007966	0.706441
-42.499227	-1.858207	1.821747	0.007949	0.706399
-43.192141	-1.870154	1.826752	0.008078	0.706127
-42.777130	-1.941050	1.831757	0.008000	0.706134
-43.530519	-1.810228	1.836762	0.008140	0.706127
-43.742731	-1.770984	1.841766	0.008179	0.706130
-43.299600	-1.849534	1.846771	0.008096	0.706132
-43.333770	-1.846376	1.851776	0.008103	0.706126
-43.326832	-1.852799	1.856781	0.008101	0.706117
-43.957993	-1.868437	1.861786	0.008218	0.705859
-43.945738	-1.868704	1.866790	0.008216	0.705864
-44.159327	-1.830146	1.871795	0.008255	0.705865
-44.451026	-1.782399	1.876800	0.008309	0.705857
-43.980127	-1.861243	1.881805	0.008221	0.705868
-44.085305	-1.848570	1.886810	0.008241	0.705856
-44.103252	-1.877369	1.891814	0.008244	0.705792
-44.770427	-1.892614	1.896819	0.008368	0.705523
-44.904875	-1.870763	1.901824	0.008392	0.705519
-45.178562	-1.818543	1.906829	0.008443	0.705527
-45.027488	-1.847902	1.911834	0.008415	0.705522
-44.803572	-1.887881	1.916838	0.008373	0.705523
-45.108415	-1.831969	1.921843	0.008429	0.705526
-45.144752	-1.876982	1.926848	0.008436	0.705423
-45.910098	-1.843052	1.931853	0.008578	0.705217
-46.046276	-1.823644	1.936858	0.008603	0.705208
-46.529603	-1.734673	1.941862	0.008693	0.705214
-45.978073	-1.834530	1.946867	0.008590	0.705212
-45.720766	-1.883215	1.951872	0.008542	0.705207
-45.907214	-1.846354	1.956877	0.008576	0.705214
-46.170963	-1.800366	1.961882	0.008625	0.705213
-46.236820	-1.939586	1.966886	0.008637	0.704909
-46.635029	-1.877608	1.971891	0.008711	0.704892
-47.206308	-1.779157	1.976896	0.008817	0.704885
-46.636570	-1.877185	1.981901	0.008711	0.704893
-46.964267	-1.824290	1.986906	0.008771	0.704882
-47.086223	-1.799277	1.991910	0.008794	0.704889
-46.882921	-1.836473	1.996915	0.008756	0.704888
-47.744107	-1.819689	2.001920	0.008916	0.704613

-47.801667	-1.823123	2.011917	0.008926	0.704587
-47.748632	-1.830683	2.021914	0.008916	0.704591
-47.396958	-1.894975	2.031910	0.008850	0.704589
-47.747853	-1.831880	2.041907	0.008914	0.704591
-47.667088	-1.847642	2.051904	0.008899	0.704590
-47.758307	-1.832161	2.061901	0.008915	0.704589
-47.767890	-1.832436	2.071898	0.008916	0.704586
-47.687848	-1.845896	2.081894	0.008901	0.704589
-47.827043	-1.821746	2.091891	0.008926	0.704588
-47.704717	-1.844025	2.101888	0.008903	0.704589
-47.760279	-1.834590	2.111885	0.008913	0.704589
-47.615423	-1.793162	2.121882	0.008885	0.704725
-46.581960	-1.896829	2.131878	0.008692	0.704888
-47.074122	-1.809637	2.141875	0.008784	0.704888
-46.506838	-1.913375	2.151872	0.008677	0.704884
-47.106166	-1.806923	2.161869	0.008788	0.704884
-46.697354	-1.881284	2.171866	0.008712	0.704882
-46.358626	-1.782398	2.181862	0.008648	0.705204
-45.960182	-1.850057	2.191859	0.008573	0.705212
-45.935847	-1.855914	2.201856	0.008568	0.705210
-46.073358	-1.831444	2.211853	0.008593	0.705211
-45.528723	-1.807401	2.221850	0.008491	0.705456
-45.192137	-1.834748	2.231846	0.008428	0.705522
-45.137242	-1.845276	2.241843	0.008418	0.705522
-45.077707	-1.855933	2.251840	0.008406	0.705523
-44.744141	-1.771088	2.261837	0.008343	0.705814
-44.296094	-1.829904	2.271834	0.008259	0.705858
-44.211603	-1.844931	2.281830	0.008243	0.705859
-44.217170	-1.820667	2.291827	0.008244	0.705907
-43.659403	-1.812596	2.301824	0.008139	0.706124
-43.568174	-1.827774	2.311821	0.008122	0.706127
-43.372538	-1.864557	2.321818	0.008085	0.706124
-43.009119	-1.832538	2.331814	0.008017	0.706320
-42.690668	-1.830005	2.341811	0.007957	0.706440
-42.634285	-1.840643	2.351808	0.007946	0.706440
-42.698634	-1.807941	2.361805	0.007957	0.706483
-41.688632	-1.857081	2.371802	0.007769	0.706747
-41.625620	-1.867072	2.381798	0.007756	0.706751
-41.463390	-1.896538	2.391795	0.007726	0.706751
-41.577190	-1.799248	2.401792	0.007746	0.706907
-40.932082	-1.829274	2.411789	0.007626	0.707078
-40.942052	-1.828552	2.421786	0.007627	0.707077
-41.027109	-1.788752	2.431782	0.007642	0.707128
-39.995171	-1.848211	2.441779	0.007449	0.707378
-40.109508	-1.828730	2.451776	0.007470	0.707378
-40.033687	-1.844741	2.461773	0.007456	0.707374
-39.556519	-1.815825	2.471770	0.007366	0.707603
-39.168830	-1.836464	2.481766	0.007293	0.707702
-39.097887	-1.850242	2.491763	0.007280	0.707700
-39.311835	-1.775834	2.501760	0.007319	0.707774
-38.400696	-1.821626	2.511757	0.007149	0.708009
-38.340199	-1.832801	2.521754	0.007137	0.708009
-38.369467	-1.827860	2.531750	0.007142	0.708010
-37.369878	-1.860593	2.541747	0.006955	0.708302
-37.226178	-1.863666	2.551744	0.006928	0.708348
-37.224170	-1.865820	2.561741	0.006927	0.708346
-37.214502	-1.867117	2.571738	0.006925	0.708348
-36.784287	-1.800946	2.581734	0.006844	0.708635
-36.293048	-1.887448	2.591731	0.006752	0.708638
-36.697645	-1.816978	2.601728	0.006827	0.708636
-36.074742	-1.830247	2.611725	0.006710	0.708833
-35.634540	-1.849961	2.621722	0.006628	0.708951
-35.708813	-1.835476	2.631718	0.006641	0.708955
-35.579636	-1.838631	2.641715	0.006617	0.708995
-35.140970	-1.783355	2.651712	0.006534	0.709264
-34.747499	-1.855943	2.661709	0.006461	0.709260
-34.958723	-1.818847	2.671706	0.006499	0.709260
-33.909328	-1.871579	2.681702	0.006304	0.709529
-34.141565	-1.798505	2.691699	0.006346	0.709594
-33.951782	-1.832486	2.701696	0.006310	0.709594
-33.678896	-1.842514	2.711693	0.006259	0.709673
-33.235474	-1.812693	2.721690	0.006176	0.709891
-32.874648	-1.876998	2.731686	0.006108	0.709892
-32.864718	-1.879121	2.741683	0.006106	0.709893
-32.646813	-1.799297	2.751680	0.006065	0.710131
-32.355786	-1.809749	2.761677	0.006010	0.710215
-32.430602	-1.795674	2.771674	0.006023	0.710217
-31.656102	-1.872409	2.781670	0.005879	0.710341
-31.136675	-1.869284	2.791667	0.005781	0.710533
-31.131927	-1.870013	2.801664	0.005780	0.710534
-31.155886	-1.867427	2.811661	0.005784	0.710532
-30.756620	-1.829710	2.821658	0.005709	0.710750
-30.260080	-1.858659	2.831654	0.005616	0.710870
-30.474467	-1.819947	2.841651	0.005655	0.710872
-30.457476	-1.799761	2.851648	0.005652	0.710919
-29.701049	-1.828054	2.861645	0.005510	0.711133
-29.602257	-1.845541	2.871642	0.005491	0.711134
-29.372647	-1.885439	2.881638	0.005448	0.711137
-29.130292	-1.799799	2.891635	0.005402	0.711395
-28.659831	-1.854327	2.901632	0.005314	0.711455
-29.102947	-1.776307	2.911629	0.005396	0.711454
-28.516776	-1.793886	2.921626	0.005287	0.711628
-27.878370	-1.841838	2.931622	0.005167	0.711760
-27.872810	-1.842711	2.941619	0.005166	0.711762
-28.033055	-1.783777	2.951616	0.005195	0.711823
-26.900054	-1.853923	2.961613	0.004983	0.712087
-27.302431	-1.781636	2.971610	0.005058	0.712089
-27.057852	-1.824000	2.981606	0.005012	0.712092
-26.551002	-1.789777	2.991603	0.004917	0.712342
-26.263576	-1.816784	3.001600	0.004863	0.712391
-26.492769	-1.777161	3.011597	0.004905	0.712389
-25.911042	-1.788916	3.021594	0.004796	0.712573
-25.247897	-1.840273	3.031590	0.004672	0.712708
-25.628498	-1.772339	3.041587	0.004742	0.712709
-25.464311	-1.765597	3.051584	0.004711	0.712781
-24.416354	-1.832093	3.061581	0.004516	0.713022
-24.563933	-1.807014	3.071578	0.004543	0.713020
-24.514106	-1.815616	3.081574	0.004533	0.713022
-24.101113	-1.764296	3.091571	0.004455	0.713271
-23.629215	-1.807161	3.101568	0.004367	0.713354
-23.652649	-1.802081	3.111565	0.004371	0.713357
-23.441180	-1.801565	3.121562	0.004331	0.713434
-22.798947	-1.807716	3.131558	0.004211	0.713651
-22.895298	-1.789487	3.141555	0.004228	0.713654
-22.721086	-1.822804	3.151552	0.004195	0.713650
-22.396799	-1.740894	3.161549	0.004134	0.713929
-22.028804	-1.787384	3.171546	0.004065	0.713968
-21.774029	-1.833284	3.181542	0.004017	0.713968
-21.777127	-1.761348	3.191539	0.004017	0.714111
-20.912441	-1.831215	3.201536	0.003856	0.714279
-21.093854	-1.799837	3.211533	0.003889	0.714278
-20.925810	-1.831701	3.221530	0.003857	0.714275
-20.180232	-1.807948	3.231526	0.003718	0.714587
-20.020784	-1.825252	3.241523	0.003688	0.714610
-19.796984	-1.866026	3.251520	0.003645	0.714609
-20.250551	-1.758687	3.261517	0.003729	0.714663
-19.292363	-1.806666	3.271514	0.003550	0.714908
-19.273972	-1.809034	3.281510	0.003546	0.714911
-19.238571	-1.815338	3.291507	0.003539	0.714912
-18.578237	-1.804887	3.301504	0.003416	0.715167
-18.562334	-1.777264	3.311501	0.003412	0.715228
-18.217581	-1.839505	3.321498	0.003348	0.715228
-18.278748	-1.788417	3.331494	0.003358	0.715308
-17.442689	-1.817825	3.341491	0.003202	0.715546
-17.224541	-1.858063	3.351488	0.003161	0.715545
-17.429831	-1.822908	3.361485	0.003199	0.715543
-16.708149	-1.854962	3.371482	0.003064	0.715735
-16.398865	-1.837777	3.381478	0.003006	0.715879
-16.366616	-1.842296	3.391475	0.002999	0.715883
-16.112388	-1.886121	3.401472	0.002951	0.715887
-15.912711	-1.847066	3.411469	0.002914	0.716036
-15.659322	-1.844114	3.421466	0.002866	0.716132
-15.693615	-1.837923	3.431462	0.002872	0.716133
-15.450451	-1.853500	3.441459	0.002826	0.716189
-14.510465	-1.890126	3.451456	0.002650	0.716449
-14.832461	-1.835843	3.461453	0.002710	0.716444
-14.751548	-1.850252	3.471450	0.002694	0.716445
-14.537162	-1.788647	3.481446	0.002654	0.716644
-13.808012	-1.863723	3.491443	0.002518	0.716753
-13.938494	-1.840200	3.501440	0.002541	0.716755
-13.779369	-1.826880	3.511437	0.002511	0.716838
-12.872354	-1.865757	3.521434	0.002342	0.717082
-12.865992	-1.868229	3.531430	0.002340	0.717080
-12.835141	-1.871508	3.541427	0.002334	0.717086
-12.454083	-1.839059	3.551424	0.002262	0.717285
-12.211280	-1.837211	3.561421	0.002216	0.717375
-12.051165	-1.865489	3.571418	0.002186	0.717377
-12.177213	-1.802125	3.581414	0.002209	0.717459
-10.930609	-1.901132	3.591411	0.001976	0.717703
-11.388900	-1.819578	3.601408	0.002061	0.717704
-11.182514	-1.857638	3.611405	0.002022	0.717702
-10.776782	-1.813551	3.621402	0.001946	0.717933
-10.298192	-1.857175	3.631398	0.001857	0.718016
-10.351108	-1.848576	3.641395	0.001866	0.718016
-10.304499	-1.810981	3.651392	0.001857	0.718107
-9.354984	-1.856987	3.661389	0.001679	0.718352
-9.342693	-1.859764	3.671386	0.001677	0.718351
-9.461081	-1.839781	3.681382	0.001698	0.718350
-8.805220	-1.863092	3.691379	0.001575	0.718536
-8.670641	-1.834279	3.701376	0.001550	0.718641
-8.437068	-1.876824	3.711373	0.001506	0.718640
-8.588142	-1.835182	3.721370	0.001533	0.718670
-7.682933	-1.850569	3.731366	0.001364	0.718959
-7.564211	-1.871509	3.741363	0.001342	0.718960
-7.675978	-1.851875	3.751360	0.001362	0.718961
-7.258052	-1.846787	3.761357	0.001284	0.719119
-6.932683	-1.829794	3.771354	0.001222	0.719268
-6.837463	-1.846429	3.781350	0.001204	0.719269
-6.594714	-1.883037	3.791347	0.001158	0.719283
-6.144678	-1.800530	3.801344	0.001074	0.719605
-5.642338	-1.893475	3.811341	0.000980	0.719599
-5.795773	-1.867531	3.821338	0.001008	0.719597
-5.700696	-1.827038	3.831334	0.000990	0.719711
-4.825914	-1.887194	3.841331	0.000826	0.719901
-4.937108	-1.869131	3.851328	0.000847	0.719898
-4.837434	-1.886518	3.861325	0.000828	0.719900
-4.492201	-1.812778	3.871322	0.000763	0.720168
-4.117197	-1.851813	3.881318	0.000692	0.720223
-4.311843	-1.816349	3.891315	0.000728	0.720226
-4.033929	-1.789628	3.901312	0.000676	0.720377
-3.414425	-1.815857	3.911309	0.000560	0.720543
-3.323257	-1.833753	3.921306	0.000542	0.720541
-3.164685	-1.846340	3.931302	0.000512	0.720573
-2.710890	-1.770307	3.941299	0.000427	0.720883
-2.496727	-1.809191	3.951296	0.000387	0.720882
-2.445204	-1.818995	3.961293	0.000377	0.720882
-2.294510	-1.755159	3.971290	0.000348	0.721061
-1.884278	-1.797804	3.981286	0.000271	0.721122
-2.023840	-1.772984	3.991283	0.000297	0.721123
-1.682185	-1.719191	4.001280	0.000232	0.721349
-1.425920	-1.720094	4.011277	0.000184	0.721438
-1.293845	-1.744201	4.021274	0.000159	0.721438
-1.314809	-1.605422	4.031270	0.000162	0.721705
-1.276591	-1.591418	4.041267	0.000155	0.721746
-1.249746	-1.513492	4.051264	0.000149	0.721910
-1.101988	-1.455923	4.061261	0.000121	0.722076
-0.875129	-1.449351	4.071258	0.000078	0.722169
-0.866385	-1.350000	4.081254	0.000076	0.722368
-0.532677	-1.363987	4.091251	0.000013	0.722458
-0.514438	-1.246133	4.101248	0.000009	0.722697
-0.477190	-1.198389	4.111245	0.000002	0.722805
-0.507852	-1.092170	4.121242	0.000007	0.723003
-0.584330	-0.969278	4.131238	0.000021	0.723219
-0.301831	-0.949414	4.141235	-0.000033	0.723357
-0.298242	-0.809100	4.151232	-0.000034	0.723634
-0.429636	-0.699829	4.161229	-0.000010	0.723804
-0.393809	-0.607024	4.171226	-0.000017	0.723999
-0.293948	-0.491348	4.181222	-0.000036	0.724261
-0.067538	-0.391285	4.191219	-0.000079	0.724537
-0.059451	-0.285930	4.201216	-0.000081	0.724747
0.043650	-0.188510	4.211213	-0.000101	0.724975
-0.156176	-0.017182	4.221210	-0.000064	0.725241
0.000000	0.159690	4.231206	-0.000094	0.725642

-0.186346	0.796043	4.236211	-0.000060	0.726820
0.152084	2.019899	4.241216	-0.000124	0.729322
0.675743	3.789078	4.246221	-0.000223	0.732935
0.740046	6.201602	4.251226	-0.000237	0.737610
1.179750	9.057751	4.256230	-0.000321	0.743231
1.793556	12.372074	4.261235	-0.000438	0.749734
2.059404	16.199764	4.266240	-0.000490	0.757028
2.713634	20.359932	4.271245	-0.000615	0.764997
3.427769	24.929437	4.276250	-0.000751	0.773653
4.188996	29.858932	4.281254	-0.000896	0.782881
4.734969	35.171572	4.286259	-0.001002	0.792618
6.145051	40.669797	4.291264	-0.001268	0.802835
7.239789	46.532988	4.296269	-0.001476	0.813462
7.964987	52.737803	4.301274	-0.001615	0.824427
9.079535	59.162259	4.306278	-0.001827	0.835737
10.493488	65.731567	4.311283	-0.002095	0.847226
11.585464	72.616122	4.316288	-0.002303	0.858987
12.404595	79.753103	4.321293	-0.002461	0.870921
13.562115	87.014952	4.326298	-0.002681	0.882990
14.870339	94.439207	4.331302	-0.002930	0.895195
15.638121	102.103747	4.336307	-0.003078	0.907461
16.530111	109.910192	4.341312	-0.003250	0.919816
17.224228	117.850499	4.346317	-0.003384	0.932158
17.957351	125.905139	4.351322	-0.003526	0.944519
18.760650	134.053834	4.356326	-0.003681	0.956878
19.485882	142.289400	4.361331	-0.003822	0.969186
20.391368	150.581381	4.366336	-0.003996	0.981467
20.936202	159.026459	4.371341	-0.004104	0.993723
21.961693	167.400676	4.376346	-0.004300	1.005848
22.957000	175.844161	4.381350	-0.004491	1.017917
23.366980	184.420413	4.386355	-0.004573	1.029887
23.999293	192.989196	4.391360	-0.004697	1.041761
25.369699	201.464332	4.396365	-0.004958	1.053547
26.175277	210.071696	4.401370	-0.005114	1.065248
26.908101	218.725180	4.406374	-0.005256	1.076866
27.920619	227.301793	4.411379	-0.005451	1.088321
28.885909	235.920411	4.416384	-0.005636	1.099701
29.637787	244.580888	4.421389	-0.005782	1.110970
30.658504	253.189942	4.426394	-0.005978	1.122118
31.916223	261.782141	4.431398	-0.006218	1.133187
32.672771	270.447522	4.436403	-0.006365	1.144132
33.247337	279.187316	4.441408	-0.006478	1.155025
33.703370	287.854719	4.446413	-0.006569	1.165704
34.203968	296.522502	4.451418	-0.006668	1.176296
35.252354	305.067550	4.456422	-0.006869	1.186758
36.222997	313.634029	4.461427	-0.007055	1.197137
37.147050	322.201215	4.466432	-0.007233	1.207418
37.525063	330.848436	4.471437	-0.007310	1.217597
38.066289	339.451381	4.476442	-0.007416	1.227673
38.963776	347.997452	4.481446	-0.007589	1.237670
39.513189	356.547109	4.486451	-0.007697	1.247524
40.326287	365.067145	4.491456	-0.007855	1.257317
40.992247	373.580947	4.496461	-0.007984	1.266999
41.404365	382.135935	4.501466	-0.008067	1.276606
41.798862	390.661856	4.506470	-0.008146	1.286105
42.284776	399.166038	4.511475	-0.008243	1.295528
42.718189	407.660400	4.516480	-0.008329	1.304862
42.987742	416.270751	4.521485	-0.008385	1.314225
43.851331	424.655118	4.526490	-0.008552	1.323386
44.592558	433.048663	4.531494	-0.008695	1.332472
44.833646	441.496313	4.536499	-0.008746	1.341465
45.111774	449.945426	4.541504	-0.008804	1.350406
45.474708	458.351720	4.546509	-0.008877	1.359258
46.009448	466.711754	4.551514	-0.008982	1.368035
46.003876	475.175327	4.556518	-0.008987	1.376769
46.306604	483.543971	4.561523	-0.009049	1.385404
46.790881	491.912210	4.566528	-0.009145	1.394015
47.358499	500.216400	4.571533	-0.009256	1.402522
47.660234	508.565568	4.576538	-0.009318	1.410979
48.002070	516.915399	4.581542	-0.009388	1.419392
48.351226	525.233897	4.586547	-0.009458	1.427726
48.593327	533.596929	4.591552	-0.009509	1.436038
48.811296	541.916201	4.596557	-0.009555	1.444255
49.421981	550.184046	4.601562	-0.009675	1.452438
49.714596	558.506956	4.606566	-0.009735	1.460578
49.927527	566.834823	4.611571	-0.009780	1.468665
50.395753	575.151972	4.616576	-0.009873	1.476738
50.847277	583.387148	4.621581	-0.009963	1.484685
51.798418	591.580470	4.626586	-0.010146	1.492628
52.328762	599.834212	4.631590	-0.010250	1.500521
52.774180	608.102461	4.636595	-0.010339	1.508372
52.797745	616.447741	4.641600	-0.010349	1.516191
52.868425	624.731950	4.646605	-0.010367	1.523920
53.493990	632.942019	4.651610	-0.010490	1.531624
53.667499	641.233382	4.656614	-0.010528	1.539298
54.058617	649.454214	4.661619	-0.010606	1.546900
54.579404	657.710456	4.666624	-0.010709	1.554517
54.827884	665.944481	4.671629	-0.010761	1.562036
54.944313	674.209945	4.676634	-0.010788	1.569529
55.417457	682.430783	4.681638	-0.010882	1.576997
55.656648	690.646820	4.686643	-0.010932	1.584392
55.982812	698.894078	4.691648	-0.010998	1.591793
56.181768	707.127092	4.696653	-0.011041	1.599128
56.401695	715.332319	4.701658	-0.011087	1.606409
56.679032	723.577793	4.706662	-0.011145	1.613700
56.998205	731.766133	4.711667	-0.011210	1.620914
57.524787	739.949756	4.716672	-0.011313	1.628120
57.805637	748.224319	4.721677	-0.011371	1.635340
58.112721	756.393468	4.726682	-0.011434	1.642440
58.624660	764.557894	4.731686	-0.011535	1.649534
59.001152	772.737625	4.736691	-0.011611	1.656592
59.272578	780.933632	4.741696	-0.011667	1.663619
59.738955	789.092983	4.746701	-0.011759	1.670612
60.353216	797.246789	4.751706	-0.011879	1.677590
60.717702	805.417413	4.756710	-0.011953	1.684521
60.660727	813.667143	4.761715	-0.011948	1.691433
61.082567	821.839585	4.766720	-0.012032	1.698316
61.421316	829.990717	4.771725	-0.012100	1.705142
61.731967	838.194247	4.776730	-0.012164	1.711981
61.833546	846.407940	4.781734	-0.012188	1.718773
61.997269	854.561177	4.786739	-0.012225	1.725497
62.470829	862.721283	4.791744	-0.012318	1.732241
62.806912	870.874481	4.796749	-0.012386	1.738935
63.623975	878.945670	4.801754	-0.012544	1.745597
64.073829	887.138433	4.806758	-0.012633	1.752286
64.386255	895.296983	4.811763	-0.012697	1.758905
64.793291	903.447714	4.816768	-0.012779	1.765504
65.072489	911.627409	4.821773	-0.012836	1.772085
65.042483	919.842196	4.826778	-0.012836	1.778632
65.702543	927.932793	4.831782	-0.012965	1.785142
66.234103	936.093885	4.836787	-0.013069	1.791667
66.673396	944.265277	4.841792	-0.013157	1.798166
66.665216	952.436052	4.846797	-0.013161	1.804586
66.867622	960.594611	4.851802	-0.013204	1.810999
67.359407	968.718198	4.856806	-0.013301	1.817397
67.549657	976.854255	4.861811	-0.013342	1.823746
67.924904	984.993010	4.866816	-0.013417	1.830097
68.254342	993.134052	4.871821	-0.013484	1.836422
68.524769	1001.265419	4.876826	-0.013540	1.842712
68.818383	1009.420679	4.881830	-0.013601	1.849000
69.275915	1017.534494	4.886835	-0.013691	1.855255
69.571595	1025.675654	4.891840	-0.013752	1.861491
69.871166	1033.814982	4.896845	-0.013813	1.867704
70.190291	1041.979768	4.901850	-0.013878	1.873919
70.705937	1050.063438	4.906854	-0.013980	1.880074
70.781531	1058.214451	4.911859	-0.014000	1.886209
71.148074	1066.352876	4.916864	-0.014073	1.892349
71.580989	1074.450850	4.921869	-0.014159	1.898445
71.874008	1082.564760	4.926874	-0.014220	1.904518
72.068652	1090.727338	4.931878	-0.014261	1.910597
72.285909	1098.856883	4.936883	-0.014307	1.916634
72.696788	1106.950167	4.941888	-0.014390	1.922647
72.674885	1115.117647	4.946893	-0.014391	1.928648
72.974556	1123.232258	4.951898	-0.014452	1.934627
73.295459	1131.347444	4.956902	-0.014518	1.940590
73.409549	1139.474526	4.961907	-0.014544	1.946521
73.632625	1147.644404	4.966912	-0.014592	1.952476
74.107964	1155.719344	4.971917	-0.014686	1.958373
74.409296	1163.795260	4.976922	-0.014747	1.964233
74.883641	1171.890138	4.981926	-0.014841	1.970108
75.330662	1179.965951	4.986931	-0.014930	1.975949
76.329603	1187.985969	4.991936	-0.015121	1.981791
76.729385	1196.111598	4.996941	-0.015201	1.987628
77.107256	1204.236140	5.001946	-0.015277	1.993444
77.586066	1212.342637	5.006950	-0.015372	1.999241
77.558680	1220.484444	5.011955	-0.015373	2.004993
77.705197	1228.630312	5.016960	-0.015405	2.010750
78.242011	1236.710585	5.021965	-0.015511	2.016485
78.599524	1244.805557	5.026970	-0.015583	2.022195
78.585030	1252.984181	5.031974	-0.015586	2.027908
78.770330	1261.116075	5.036979	-0.015626	2.033594
79.225413	1269.175426	5.041984	-0.015716	2.039241
79.411023	1277.271148	5.046989	-0.015756	2.044870
79.699001	1285.371162	5.051994	-0.015815	2.050497
80.020355	1293.479033	5.056998	-0.015881	2.056118
80.466049	1301.541136	5.062003	-0.015969	2.061704
80.615458	1309.669224	5.067008	-0.016003	2.067290
80.703580	1317.805512	5.072013	-0.016025	2.072860
81.000293	1325.881790	5.077018	-0.016085	2.078396
81.209878	1333.976668	5.082022	-0.016130	2.083920
81.531572	1342.050870	5.087027	-0.016195	2.089428
81.887649	1350.163378	5.092032	-0.016267	2.094949
82.139568	1358.254983	5.097037	-0.016320	2.100432
82.501309	1366.328583	5.102042	-0.016393	2.105899
82.990173	1374.448179	5.107046	-0.016489	2.111395
83.013003	1382.602884	5.112051	-0.016499	2.116855
83.460022	1390.640265	5.117056	-0.016588	2.122264
83.726370	1398.705503	5.122061	-0.016643	2.127660
83.990012	1406.801237	5.127066	-0.016698	2.133062
84.580818	1414.844790	5.132070	-0.016813	2.138447
84.770397	1422.933256	5.137075	-0.016854	2.143810
85.321062	1430.991387	5.142080	-0.016962	2.149173
85.451645	1439.140600	5.147085	-0.016992	2.154544
85.609549	1447.218188	5.152090	-0.017027	2.159857
85.891391	1455.301233	5.157094	-0.017085	2.165171
86.251930	1463.360591	5.162099	-0.017157	2.170465
86.720450	1471.448800	5.167104	-0.017250	2.175774
86.640281	1479.577525	5.172109	-0.017241	2.181046
86.923689	1487.645132	5.177114	-0.017299	2.186299
87.483842	1495.717119	5.182118	-0.017409	2.191568
87.690785	1503.816484	5.187123	-0.017453	2.196809
87.942883	1511.896425	5.192128	-0.017506	2.202029
88.241422	1519.954363	5.197133	-0.017567	2.207227
88.507201	1528.042245	5.202138	-0.017622	2.212429
88.716606	1536.154850	5.207142	-0.017666	2.217629
88.939946	1544.196902	5.212147	-0.017713	2.222774
89.226002	1552.292233	5.217152	-0.017772	2.227946
89.479082	1560.391008	5.222157	-0.017825	2.233105
89.919012	1568.425034	5.227162	-0.017912	2.238228
90.281971	1576.500425	5.232166	-0.017985	2.243358
90.424879	1584.577374	5.237171	-0.018017	2.248458
90.959663	1592.648051	5.242176	-0.018123	2.253577
91.311599	1600.725262	5.247181	-0.018194	2.258672
91.486564	1608.791841	5.252186	-0.018232	2.263734
91.967952	1616.865418	5.257190	-0.018327	2.268815
92.521949	1624.997081	5.262195	-0.018436	2.273927
92.623043	1633.079794	5.267200	-0.018460	2.278958
92.765801	1641.139415	5.272205	-0.018492	2.283968
92.963383	1649.201706	5.277210	-0.018534	2.288973
93.443183	1657.272557	5.282214	-0.018629	2.293996
93.445286	1665.349993	5.287219	-0.018635	2.298971
93.720204	1673.412573	5.292224	-0.018692	2.303950
93.852296	1681.508809	5.297229	-0.018722	2.308926
94.504155	1689.547376	5.302234	-0.018849	2.313900
94.853939	1697.603283	5.307238	-0.018920	2.318849
95.224355	1705.645880	5.312243	-0.018994	2.323780
95.485002	1713.734669	5.317248	-0.019048	2.328720
95.697895	1721.827493	5.322253	-0.019093	2.333648
96.013892	1729.895952	5.327258	-0.019158	2.338559
96.125670	1737.976210	5.332262	-0.019184	2.343451
96.130088	1746.056370	5.337267	-0.019190	2.348323
96.601437	1754.148573	5.342272	-0.019284	2.353230
97.291499	1762.138654	5.347277	-0.019418	2.358084
97.794659	1770.161503	5.352282	-0.019517	2.362931
98.430440	1778.194022	5.357286	-0.019641	2.367786
98.553655	1786.304047	5.362291	-0.019669	2.372635
98.890110	1794.380593	5.367296	-0.019737	2.377471
98.931402	1802.481602	5.372301	-0.019751	2.382289
99.380938	1810.520122	5.377306	-0.019840	2.387092
99.717225	1818.612732	5.382310	-0.019908	2.391909
99.956260	1826.684351	5.387315	-0.019958	2.396695
100.111690	1834.765136	5.392320	-0.019992	2.401471
100.927369	1842.750557	5.397325	-0.020150	2.406233
102.738773	1850.648947	5.402330	-0.020493	2.411012
103.175990	1858.778940	5.407334	-0.020579	2.415810
103.665859	1866.839592	5.412339	-0.020676	2.420562
103.833910	1874.963302	5.417344	-0.020713	2.425316
103.994613	1883.083122	5.422349	-0.020749	2.430058
104.156408	1891.239202	5.427354	-0.020784	2.434812
104.337864	1899.301568	5.432358	-0.020824	2.439504
104.372028	1907.358226	5.437363	-0.020835	2.444173
104.891167	1915.387138	5.442368	-0.020938	2.448853
105.095507	1923.461142	5.447373	-0.020981	2.453526
105.413158	1931.500288	5.452378	-0.021046	2.458179
105.680113	1939.566405	5.457382	-0.021101	2.462835
105.791462	1947.625527	5.462387	-0.021127	2.467466
106.158008	1955.699609	5.467392	-0.021201	2.472116
106.414557	1963.755888	5.472397	-0.021254	2.476739
106.576777	1971.805417	5.477402	-0.021290	2.481342
107.026361	1979.852732	5.482406	-0.021379	2.485957
107.162770	1987.914927	5.487411	-0.021410	2.490549
107.495140	1996.000338	5.492416	-0.021478	2.495159
107.821187	2004.043511	5.497421	-0.021544	2.499737
107.922327	2012.092514	5.502426	-0.021568	2.504293
108.100305	2020.179587	5.507430	-0.021607	2.508868
108.287768	2028.266170	5.512435	-0.021647	2.513435
108.572483	2036.295604	5.517440	-0.021706	2.517968
108.930451	2044.320553	5.522445	-0.021778	2.522496
109.407450	2052.338213	5.527450	-0.021872	2.527020
109.865660	2060.398665	5.532454	-0.021963	2.531559
109.702222	2068.500333	5.537459	-0.021938	2.536068
110.081505	2076.531990	5.542464	-0.022014	2.540569
110.488849	2084.562760	5.547469	-0.022096	2.545063
110.752956	2092.619435	5.552474	-0.022150	2.549553
111.037417	2100.713848	5.557478	-0.022209	2.554058
111.281908	2108.745879	5.562483	-0.022260	2.558517
111.528305	2116.794954	5.567488	-0.022311	2.562979
111.768497	2124.850210	5.572493	-0.022362	2.567435
111.888083	2132.928299	5.577498	-0.022389	2.571888
112.437198	2140.974630	5.582502	-0.022497	2.576345
112.617471	2149.008381	5.587507	-0.022536	2.580762
112.822012	2157.073521	5.592512	-0.022580	2.585190
113.044845	2165.144612	5.597517	-0.022627	2.589616
113.327472	2173.373698	5.602522	-0.022685	2.594124
113.993190	2181.346755	5.607526	-0.022815	2.598510
114.077132	2189.346776	5.612531	-0.022836	2.602865
114.328161	2197.374854	5.617536	-0.022888	2.607238
114.628701	2205.422527	5.622541	-0.022949	2.611619
114.719430	2213.470956	5.627546	-0.022972	2.615978
115.191897	2221.477156	5.632550	-0.023065	2.620332
115.297457	2229.513398	5.637555	-0.023090	2.624671
115.627378	2237.565185	5.642560	-0.023157	2.629026
115.990733	2245.626696	5.647565	-0.023230	2.633381
116.272722	2253.659954	5.652570	-0.023288	2.637709
116.492580	2261.716558	5.657574	-0.023335	2.642037
116.721989	2269.749980	5.662579	-0.023383	2.646347
117.121616	2277.792751	5.667584	-0.023463	2.650666
117.329839	2285.887268	5.672589	-0.023507	2.654993
117.387206	2293.920171	5.677594	-0.023524	2.659270
117.766183	2301.975635	5.682598	-0.023600	2.663573
118.066865	2310.009114	5.687603	-0.023661	2.667852
118.176329	2318.116117	5.692608	-0.023687	2.672151
118.307704	2326.183342	5.697613	-0.023717	2.676424
118.829119	2334.168297	5.702618	-0.023820	2.680671
119.130653	2342.216564	5.707622	-0.023881	2.684931
119.186302	2350.249896	5.712627	-0.023897	2.689160
119.643740	2358.309906	5.717632	-0.023988	2.693422
119.817441	2366.368872	5.722637	-0.024026	2.697659
120.009900	2374.409119	5.727642	-0.024067	2.701881
120.510621	2382.423256	5.732646	-0.024166	2.706101
120.664187	2390.486429	5.737651	-0.024200	2.710319
121.036207	2398.549909	5.742656	-0.024275	2.714544
121.270659	2406.579554	5.747661	-0.024324	2.718736
121.381887	2414.624406	5.752666	-0.024350	2.722922
121.518351	2422.685934	5.757670	-0.024381	2.727112
121.617532	2430.744470	5.762675	-0.024405	2.731291
122.070033	2438.789186	5.767680	-0.024495	2.735479
122.476762	2446.790195	5.772685	-0.024576	2.739635
122.542375	2454.839706	5.777690	-0.024594	2.743788
122.850953	2462.926182	5.782694	-0.024657	2.747969
123.092028	2470.987523	5.787699	-0.024707	2.752127
123.467567	2479.074597	5.792704	-0.024783	2.756299
123.672126	2487.097285	5.797709	-0.024826	2.760422
124.051671	2495.068811	5.802714	-0.024902	2.764523
124.336230	2503.116734	5.807718	-0.024961	2.768652
124.469437	2511.176774	5.812723	-0.024991	2.772771
124.807519	2519.232327	5.817728	-0.025060	2.776894
125.040603	2527.274813	5.822733	-0.025108	2.780998
125.251945	2535.286934	5.827738	-0.025153	2.785079
125.585621	2543.339856	5.832742	-0.025221	2.789182
125.846596	2551.400304	5.837747	-0.025275	2.793278
125.986460	2559.444736	5.842752	-0.025307	2.797353
126.253634	2567.478227	5.847757	-0.025362	2.801424
126.481566	2575.492141	5.852762	-0.025410	2.805477
126.714349	2583.538324	5.857766	-0.025459	2.809541
126.583443	2591.634385	5.862771	-0.025440	2.813602
126.984397	2599.664843	5.867776	-0.025520	2.817656
127.412987	2607.673382	5.872781	-0.025605	2.821694
127.595167	2615.727449	5.877786	-0.025645	2.825736
127.677115	2623.799602	5.882790	-0.025665	2.829774
127.976435	2631.844157	5.887795	-0.025727	2.833806
128.358730	2639.868326	5.892800	-0.025803	2.837826
128.395107	2647.917655	5.897805	-0.025816	2.841833
128.583685	2655.917727	5.902810	-0.025856	2.845819
129.096223	2663.950370	5.907814	-0.025957	2.849834
129.048716	2672.039652	5.912819	-0.025954	2.853839
129.367633	2680.069256	5.917824	-0.026019	2.857830
129.558928	2688.116423	5.922829	-0.026060	2.861817
129.662474	2696.140470	5.927834	-0.026085	2.865782
129.964424	2704.181955	5.932838	-0.026146	2.869761
129.943964	2712.275984	5.937843	-0.026148	2.873742
129.893714	2720.318442	5.942848	-0.026144	2.877691
130.182995	2728.327007	5.947853	-0.026204	2.881637
130.441459	2736.352701	5.952858	-0.026257	2.885584
131.010215	2744.352446	5.957862	-0.026369	2.889529
130.917495	2752.459302	5.962867	-0.026357	2.893486
131.220416	2760.493005	5.967872	-0.026419	2.897423
131.530789	2768.508134	5.972877	-0.026482	2.901345
131.798877	2776.538959	5.977882	-0.026538	2.905268
132.269143	2784.579059	5.982886	-0.026631	2.909201
132.536314	2792.695793	5.987891	-0.026686	2.913155
132.819814	2800.727805	5.992896	-0.026744	2.917063
132.920049	2808.743739	5.997901	-0.026768	2.920948
133.290705	2816.702658	6.002906	-0.026843	2.924815
133.553138	2824.769573	6.007910	-0.026897	2.928723
133.731021	2832.797670	6.012915	-0.026936	2.932603
133.983102	2840.854373	6.017920	-0.026988	2.936495
134.250937	2848.893556	6.022925	-0.027044	2.940375
134.064407	2856.919961	6.027930	-0.027014	2.944219
134.519474	2864.957602	6.032934	-0.027105	2.948097
134.866091	2872.999543	6.037939	-0.027175	2.951967
135.086077	2881.041732	6.042944	-0.027221	2.955824
135.284863	2889.070676	6.047949	-0.027264	2.959670
135.467709	2897.095518	6.052954	-0.027303	2.963507
135.985710	2905.105370	6.057958	-0.027405	2.967350
135.897050	2913.193538	6.062963	-0.027394	2.971194
136.018590	2921.263736	6.067968	-0.027422	2.975035
136.596852	2929.249578	6.072973	-0.027536	2.978854
136.750816	2937.274074	6.077978	-0.027570	2.982665
136.958649	2945.334211	6.082982	-0.027614	2.986491
137.226019	2953.364113	6.087987	-0.027669	2.990300
137.484819	2961.450968	6.092992	-0.027723	2.994131
137.617759	2969.478827	6.097997	-0.027753	2.997923
137.561707	2977.509691	6.103002	-0.027748	3.001702
137.758275	2985.551253	6.108006	-0.027790	3.005494
137.645905	2993.568424	6.113011	-0.027775	3.009255
138.190387	3001.591166	6.118016	-0.027882	3.013045
138.605953	3009.611818	6.123021	-0.027965	3.016824
138.613362	3017.681460	6.128026	-0.027972	3.020601
138.722099	3025.697156	6.133030	-0.027997	3.024352
138.960322	3033.716061	6.138035	-0.028047	3.028107
139.215708	3041.782800	6.143040	-0.028100	3.031880
139.368980	3049.840144	6.148045	-0.028134	3.035640
139.648362	3057.813880	6.153050	-0.028192	3.039361
140.286147	3065.855959	6.158054	-0.028316	3.043127
140.173707	3073.904344	6.163059	-0.028301	3.046856
140.359399	3081.939219	6.168064	-0.028341	3.050587
140.652548	3089.980406	6.173069	-0.028401	3.054323
140.668861	3098.017445	6.178074	-0.028409	3.058038
140.916026	3106.075124	6.183078	-0.028461	3.061770
141.041130	3114.081404	6.188083	-0.028490	3.065467
141.287291	3122.115586	6.193088	-0.028541	3.069178
141.650901	3130.216255	6.198093	-0.028614	3.072921
141.648665	3138.253370	6.203098	-0.028619	3.076613
141.972123	3146.276609	6.208102	-0.028685	3.080310
142.543790	3154.215659	6.213107	-0.028797	3.083975
142.409061	3162.292544	6.218112	-0.028777	3.087666
142.827916	3170.312900	6.223117	-0.028861	3.091352
142.920916	3178.356042	6.228122	-0.028884	3.095029
143.280091	3186.391627	6.233126	-0.028956	3.098710
143.498285	3194.407221	6.238131	-0.029002	3.102372
143.716428	3202.437215	6.243136	-0.029048	3.106035
143.846984	3210.487626	6.248141	-0.029078	3.109700
143.781233	3218.576142	6.253146	-0.029071	3.113369
144.081972	3226.589446	6.258150	-0.029133	3.117016
144.153915	3234.604684	6.263155	-0.029152	3.120649
144.499833	3242.584174	6.268160	-0.029222	3.124274
144.703652	3250.645951	6.273165	-0.029265	3.127925
144.813458	3258.670478	6.278170	-0.029291	3.131551
145.138842	3266.730931	6.283174	-0.029357	3.135199
144.977957	3274.754438	6.288179	-0.029333	3.138804
145.377320	3282.782777	6.293184	-0.029413	3.142432
145.631539	3290.816053	6.298189	-0.029465	3.146052
145.709304	3298.836990	6.303194	-0.029485	3.149654
146.119219	3306.907917	6.308198	-0.029567	3.153289
146.419169	3314.922322	6.313203	-0.029629	3.156890
146.448153	3322.954219	6.318208	-0.029639	3.160482
146.557516	3330.962996	6.323213	-0.029665	3.164064
146.917491	3338.968540	6.328218	-0.029738	3.167651
147.229215	3347.024464	6.333222	-0.029801	3.171254
147.249155	3355.095402	6.338227	-0.029811	3.174847
147.736493	3363.078509	6.343232	-0.029907	3.178417
147.985494	3371.116953	6.348237	-0.029959	3.181997
148.087846	3379.160334	6.353242	-0.029983	3.185569
148.414789	3387.187082	6.358246	-0.030050	3.189140
148.798293	3395.228887	6.363251	-0.030127	3.192715
148.828509	3403.283187	6.368256	-0.030138	3.196277
149.098404	3411.284086	6.373261	-0.030193	3.199821
149.362552	3419.295251	6.378266	-0.030248	3.203366
149.683109	3427.334900	6.383270	-0.030313	3.206922
149.955368	3435.352714	6.388275	-0.030369	3.210462
150.180800	3443.425860	6.393280	-0.030417	3.214020
150.175047	3451.483595	6.398285	-0.030421	3.217558
150.321491	3459.493181	6.403290	-0.030454	3.221078
150.622547	3467.505668	6.408294	-0.030516	3.224601
150.825098	3475.537002	6.413299	-0.030559	3.228125
151.163897	3483.589508	6.418304	-0.030628	3.231659
151.268030	3491.677870	6.423309	-0.030652	3.235196
151.196121	3499.658320	6.428314	-0.030645	3.238674
151.547112	3507.666872	6.433318	-0.030715	3.242178
151.911671	3515.650002	6.438323	-0.030789	3.245668
152.042293	3523.662802	6.443328	-0.030819	3.249157
152.283092	3531.743169	6.448333	-0.030869	3.252677
152.507336	3539.781382	6.453338	-0.030916	3.256174
152.732124	3547.787942	6.458342	-0.030964	3.259653
152.941048	3555.809677	6.463347	-0.031008	3.263134
152.860104	3563.878860	6.468352	-0.030998	3.266621
153.340199	3571.895342	6.473357	-0.031093	3.270103
153.652443	3579.948915	6.478362	-0.031157	3.273591
153.664568	3587.995740	6.483366	-0.031165	3.277060
153.743630	3596.016753	6.488371	-0.031185	3.280518
153.969902	3603.999561	6.493376	-0.031232	3.283961
154.241432	3612.038388	6.498381	-0.031289	3.287426
154.315660	3620.078132	6.503386	-0.031308	3.290880
154.456131	3628.147367	6.508390	-0.031340	3.294346
154.737850	3636.130844	6.513395	-0.031397	3.297776
154.782850	3644.178991	6.518400	-0.031411	3.301222
155.050938	3652.190819	6.523405	-0.031467	3.304657
155.166859	3660.238571	6.528410	-0.031494	3.308098
155.534586	3668.311931	6.533414	-0.031568	3.311556
155.483392	3676.332103	6.538419	-0.031564	3.314972
155.897153	3684.318660	6.543424	-0.031646	3.318388
156.177625	3692.332763	6.548429	-0.031704	3.321806
156.224402	3700.311144	6.553434	-0.031718	3.325197
156.488619	3708.366178	6.558438	-0.031773	3.328626
156.862553	3716.372872	6.563443	-0.031848	3.332034
157.102735	3724.453499	6.568448	-0.031898	3.335465
157.170600	3732.469752	6.573453	-0.031916	3.338859
157.357207	3740.449120	6.578458	-0.031957	3.342238
157.511178	3748.527538	6.583462	-0.031991	3.345655
157.642252	3756.542221	6.588467	-0.032021	3.349040
157.862427	3764.616681	6.593472	-0.032067	3.352450
158.219704	3772.670572	6.598477	-0.032139	3.355853
158.343267	3780.615518	6.603482	-0.032168	3.359198
158.434665	3788.670857	6.608486	-0.032190	3.362585
158.689682	3796.689820	6.613491	-0.032243	3.365959
158.920620	3804.713058	6.618496	-0.032292	3.369331
159.383696	3812.786542	6.623501	-0.032384	3.372729
159.380304	3820.828234	6.628506	-0.032388	3.376093
159.501775	3828.828481	6.633510	-0.032417	3.379441
159.874908	3836.835591	6.638515	-0.032491	3.382798
160.004981	3844.885624	6.643520	-0.032521	3.386160
160.090045	3852.905548	6.648525	-0.032543	3.389505
160.416725	3860.966376	6.653530	-0.032609	3.392872
160.546359	3869.055679	6.658534	-0.032639	3.396241
160.780408	3877.005995	6.663539	-0.032688	3.399552
160.709782	3884.997931	6.668544	-0.032680	3.402866
160.813274	3893.048647	6.673549	-0.032705	3.406208
161.186006	3901.028367	6.678554	-0.032780	3.409527
161.289691	3909.094990	6.683558	-0.032804	3.412868
161.350392	3917.144426	6.688563	-0.032821	3.416198
161.343061	3925.143847	6.693568	-0.032825	3.419502
161.788541	3933.132603	6.698573	-0.032914	3.422814
162.037635	3941.170470	6.703578	-0.032966	3.426135
162.265717	3949.208885	6.708582	-0.033014	3.429453
162.504225	3957.251310	6.713587	-0.033064	3.432770
162.899306	3965.286567	6.718592	-0.033143	3.436086
163.220799	3973.257421	6.723597	-0.033208	3.439370
163.483081	3981.288833	6.728602	-0.033262	3.442673
163.845054	3989.318483	6.733606	-0.033335	3.445976
163.850854	3997.372614	6.738611	-0.033342	3.449274
164.045747	4005.432188	6.743616	-0.033384	3.452577
164.330397	4013.483947	6.748621	-0.033442	3.455877
164.261438	4021.474766	6.753626	-0.033435	3.459137
164.486560	4029.509277	6.758630	-0.033482	3.462421
164.711883	4037.523917	6.763635	-0.033530	3.465694
164.990888	4045.556547	6.768640	-0.033587	3.468973
165.025223	4053.631729	6.773645	-0.033599	3.472258
165.277982	4061.651901	6.778650	-0.033651	3.475525
165.652666	4069.623929	6.783654	-0.033727	3.478773
165.769100	4077.648618	6.788659	-0.033754	3.482031
165.816083	4085.653975	6.793664	-0.033768	3.485276
166.059076	4093.706213	6.798669	-0.033819	3.488544
166.198387	4101.721723	6.803674	-0.033850	3.491790
166.284062	4109.769055	6.808678	-0.033872	3.495044
166.536884	4117.767570	6.813683	-0.033924	3.498280
166.904064	4125.765499	6.818688	-0.033998	3.501517
167.060787	4133.791207	6.823693	-0.034033	3.504756
167.146027	4141.843140	6.828698	-0.034054	3.507999
167.397494	4149.884307	6.833702	-0.034107	3.511241
167.519079	4157.908043	6.838707	-0.034135	3.514468
167.678662	4165.936301	6.843712	-0.034170	3.517696
167.911279	4173.947727	6.848717	-0.034219	3.520916
167.945722	4181.917038	6.853722	-0.034231	3.524110
168.174153	4189.990399	6.858726	-0.034279	3.527349
168.122085	4198.054345	6.863731	-0.034274	3.530572
168.554355	4206.052183	6.868736	-0.034360	3.533781
168.553775	4214.136393	6.873741	-0.034366	3.537008
168.621146	4222.128891	6.878746	-0.034384	3.540198
168.935266	4230.132804	6.883750	-0.034448	3.543397
169.193075	4238.147542	6.888755	-0.034501	3.546595
169.518258	4246.156745	6.893760	-0.034567	3.549791
169.694162	4254.308652	6.898765	-0.034606	3.553035
169.859097	4262.323374	6.903770	-0.034642	3.556222
170.063327	4270.286544	6.908774	-0.034685	3.559387
170.337071	4278.284065	6.913779	-0.034742	3.562565
170.257753	4286.311784	6.918784	-0.034733	3.565741
170.597352	4294.337876	6.923789	-0.034801	3.568926
170.428232	4302.397617	6.928794	-0.034775	3.572107
170.519056	4310.422485	6.933798	-0.034798	3.575278
170.778008	4318.394741	6.938803	-0.034851	3.578431
170.954551	4326.427700	6.943808	-0.034890	3.581603
171.350488	4334.424161	6.948813	-0.034969	3.584764
171.378813	4342.449758	6.953818	-0.034980	3.587923
171.537920	4350.516687	6.958822	-0.035015	3.591099
171.824885	4358.513232	6.963827	-0.035074	3.594248
172.116260	4366.526160	6.968832	-0.035134	3.597401
172.454329	4374.558841	6.973837	-0.035202	3.600560
172.399823	4382.544699	6.978842	-0.035197	3.603687
172.606240	4390.586690	6.983846	-0.035241	3.606840
172.858227	4398.614208	6.988851	-0.035294	3.609987
172.856368	4406.666862	6.993856	-0.035299	3.613133
173.242624	4414.719884	6.998861	-0.035376	3.616288
173.491412	4422.676909	7.003866	-0.035428	3.619398
173.568427	4430.743550	7.008870	-0.035448	3.622544
173.725723	4438.766692	7.013875	-0.035483	3.625672
174.081094	4446.777360	7.018880	-0.035554	3.628798
174.370187	4454.835890	7.023885	-0.035614	3.631938
174.211349	4462.877206	7.028890	-0.035590	3.635057
174.593056	4470.874976	7.033894	-0.035666	3.638170
175.026301	4478.908437	7.038899	-0.035752	3.641296
174.904836	4486.878421	7.043904	-0.035735	3.644380
175.284812	4494.932785	7.048909	-0.035812	3.647508
175.498115	4502.934595	7.053914	-0.035857	3.650607
175.536503	4511.011866	7.058918	-0.035869	3.653729
175.480485	4519.036972	7.063923	-0.035864	3.656825
175.725561	4527.021656	7.068928	-0.035916	3.659912
175.997444	4535.060818	7.073933	-0.035972	3.663017
175.909379	4543.106131	7.078938	-0.035961	3.666112
176.164390	4551.104222	7.083942	-0.036014	3.669196
176.510226	4559.137183	7.088947	-0.036084	3.672293
176.675881	4567.155825	7.093952	-0.036120	3.675376
176.735593	4575.181041	7.098957	-0.036137	3.678458
176.920035	4583.180266	7.103962	-0.036176	3.681529
177.358296	4591.214233	7.108966	-0.036264	3.684618
177.347893	4599.253055	7.113971	-0.036267	3.687695
177.521877	4607.268443	7.118976	-0.036305	3.690765
177.861439	4615.331174	7.123981	-0.036374	3.693854
177.855401	4623.305718	7.128986	-0.036378	3.696899
178.000738	4631.335875	7.133990	-0.036411	3.699966
178.079193	4639.327969	7.138995	-0.036431	3.703014
178.306809	4647.368646	7.144000	-0.036479	3.706082
178.600614	4655.409335	7.149005	-0.036539	3.709149
178.733055	4663.463975	7.154010	-0.036569	3.712215
178.856174	4671.543206	7.159014	-0.036597	3.715287
179.078749	4679.515824	7.164019	-0.036644	3.718319
179.222321	4687.514944	7.169024	-0.036677	3.721357
179.458325	4695.479321	7.174029	-0.036726	3.724381
179.426494	4703.483852	7.179034	-0.036726	3.727411
179.544176	4711.544826	7.184038	-0.036753	3.730464
179.873674	4719.567648	7.189043	-0.036820	3.733504
180.211306	4727.564401	7.194048	-0.036888	3.736533
180.240958	4735.603743	7.199053	-0.036899	3.739568
180.391055	4743.599008	7.204058	-0.036933	3.742587
180.749745	4751.630851	7.209062	-0.037005	3.745621
180.735345	4759.692648	7.214067	-0.037008	3.748656
181.000215	4767.722027	7.219072	-0.037063	3.751683
181.329735	4775.757330	7.224077	-0.037129	3.754711
181.398468	4783.746366	7.229082	-0.037148	3.757713
181.459404	4791.822206	7.234086	-0.037165	3.760745
181.535098	4799.783750	7.239091	-0.037184	3.763733
181.679184	4807.823330	7.244096	-0.037216	3.766748
181.769271	4815.860204	7.249101	-0.037239	3.769759
182.006076	4823.857889	7.254106	-0.037288	3.772756
182.383136	4831.937103	7.259110	-0.037364	3.775784
182.238857	4839.939076	7.264115	-0.037343	3.778770
182.462814	4847.977029	7.269120	-0.037390	3.781774
182.861845	4855.943122	7.274125	-0.037470	3.784754
182.941300	4863.967493	7.279130	-0.037490	3.787745
183.022435	4872.058554	7.284134	-0.037511	3.790759
183.198550	4880.063970	7.289139	-0.037549	3.793741
183.702905	4888.091607	7.294144	-0.037648	3.796736
183.670436	4896.072585	7.299149	-0.037648	3.799699
183.556702	4904.078880	7.304154	-0.037632	3.802668
184.013988	4912.055352	7.309158	-0.037723	3.805636
184.049088	4920.102569	7.314163	-0.037735	3.808618
184.010933	4928.166292	7.319168	-0.037733	3.811603
184.327846	4936.203034	7.324173	-0.037798	3.814583
184.507935	4944.169637	7.329178	-0.037837	3.817532
184.627910	4952.189078	7.334182	-0.037864	3.820496
184.786827	4960.190566	7.339187	-0.037899	3.823453
184.826239	4968.266998	7.344192	-0.037912	3.826432
185.113371	4976.279659	7.349197	-0.037971	3.829391
185.378908	4984.301575	7.354202	-0.038026	3.832350
185.580157	4992.315636	7.359206	-0.038069	3.835303
185.626519	5000.367663	7.364211	-0.038083	3.838264
185.648807	5008.351626	7.369216	-0.038093	3.841198
186.187249	5016.340803	7.374221	-0.038199	3.844141
186.493946	5024.351015	7.379226	-0.038261	3.847086
186.466703	5032.410839	7.384230	-0.038262	3.850039
186.605737	5040.456521	7.389235	-0.038293	3.852988
186.781097	5048.494476	7.394240	-0.038331	3.855933
186.836504	5056.533321	7.399245	-0.038347	3.858874
186.934361	5064.524708	7.404250	-0.038371	3.861796
187.435437	5072.519779	7.409254	-0.038470	3.864725
187.446575	5080.590693	7.414259	-0.038477	3.867670
187.411283	5088.592332	7.419264	-0.038476	3.870586
187.677045	5096.838328	7.424269	-0.038531	3.873595
187.907794	5104.825892	7.429274	-0.038580	3.876507
188.149852	5112.707327	7.434278	-0.038630	3.879378
188.173534	5120.700949	7.439283	-0.038640	3.882284
188.473521	5128.715915	7.444288	-0.038701	3.885200
188.642765	5136.734533	7.449293	-0.038738	3.888113
188.711283	5144.736165	7.454298	-0.038757	3.891016
189.110468	5152.778053	7.459302	-0.038836	3.893938
189.183215	5160.791589	7.464307	-0.038855	3.896841
189.442525	5168.781500	7.469312	-0.038909	3.899736
189.617278	5176.846678	7.474317	-0.038947	3.902655
189.653655	5184.847374	7.479322	-0.038960	3.905546
189.772914	5192.884329	7.484326	-0.038987	3.908450
189.889228	5200.898033	7.489331	-0.039014	3.911343
190.182381	5208.900826	7.494336	-0.039074	3.914233
190.480937	5216.924130	7.499341	-0.039136	3.917128
190.548785	5224.900210	7.504346	-0.039154	3.920000
190.847349	5232.939906	7.509350	-0.039215	3.922897
191.044555	5240.956057	7.514355	-0.039257	3.925781
191.191838	5248.946799	7.519360	-0.039290	3.928654
191.348969	5257.005627	7.524365	-0.039325	3.931548
191.557235	5265.035682	7.529370	-0.039369	3.934431
192.029191	5273.053329	7.534374	-0.039462	3.937313
191.997613	5281.045400	7.539379	-0.039462	3.940174
192.303882	5289.039633	7.544384	-0.039524	3.943039
192.559010	5297.093883	7.549389	-0.039577	3.945924
192.468031	5305.092473	7.554394	-0.039566	3.948780
192.892259	5313.172210	7.559398	-0.039650	3.951671
192.976450	5321.239613	7.564403	-0.039672	3.954551
192.998327	5329.206452	7.569408	-0.039681	3.957391
193.054021	5337.219479	7.574413	-0.039697	3.960247
193.288129	5345.175329	7.579418	-0.039746	3.963083
193.497891	5353.208393	7.584422	-0.039791	3.965944
193.560300	5361.249124	7.589427	-0.039808	3.968803
193.765762	5369.249312	7.594432	-0.039852	3.971648
194.192676	5377.321391	7.599437	-0.039937	3.974520
194.129113	5385.309053	7.604442	-0.039930	3.977352
194.415278	5393.313268	7.609446	-0.039989	3.980194
194.535841	5401.340783	7.614451	-0.040017	3.983039
194.581883	5409.379335	7.619456	-0.040031	3.985885
194.814942	5417.410564	7.624461	-0.040080	3.988729
195.113663	5425.427805	7.629466	-0.040141	3.991567
195.320425	5433.486956	7.634470	-0.040185	3.994416
195.459920	5441.498400	7.639475	-0.040216	3.997246
195.537150	5449.496288	7.644480	-0.040236	4.000068
195.617410	5457.522769	7.649485	-0.040257	4.002897
195.600369	5465.515917	7.654490	-0.040259	4.005712
195.651419	5473.553332	7.659494	-0.040274	4.008541
195.986921	5481.593464	7.664499	-0.040342	4.011374
196.109347	5489.608950	7.669504	-0.040370	4.014192
196.303938	5497.672280	7.674509	-0.040412	4.017027
196.717349	5505.601761	7.679514	-0.040494	4.019815
197.300405	5513.651473	7.684518	-0.040609	4.022647
197.471188	5521.683312	7.689523	-0.040646	4.025464
197.564696	5529.719773	7.694528	-0.040669	4.028280
197.981779	5537.745153	7.699533	-0.040752	4.031094
198.036258	5545.858121	7.704538	-0.040768	4.033932
198.187382	5553.855577	7.709542	-0.040801	4.036728
198.320947	5561.761014	7.714547	-0.040832	4.039491
198.538976	5569.793626	7.719552	-0.040878	4.042297
198.727843	5577.797332	7.724557	-0.040918	4.045090
198.605196	5585.812671	7.729562	-0.040901	4.047881
199.185331	5593.855016	7.734566	-0.041014	4.050690
199.139365	5601.893547	7.739571	-0.041011	4.053487
199.231065	5609.888760	7.744576	-0.041034	4.056268
199.412781	5617.892057	7.749581	-0.041073	4.059052
199.601340	5625.931230	7.754586	-0.041114	4.061846
199.713001	5633.919787	7.759590	-0.041140	4.064619
199.923154	5641.971966	7.764595	-0.041185	4.067414
200.253909	5649.953661	7.769600	-0.041252	4.070185
200.436460	5658.077731	7.774605	-0.041291	4.073001
200.804280	5666.061036	7.779610	-0.041365	4.075768
201.020905	5674.030715	7.784614	-0.041411	4.078527
201.055743	5682.052020	7.789619	-0.041423	4.081300
201.039590	5690.038324	7.794624	-0.041426	4.084057
201.380535	5698.110006	7.799629	-0.041495	4.086847
201.493913	5706.072251	7.804634	-0.041521	4.089595
201.346350	5714.148011	7.809638	-0.041499	4.092376
201.441862	5722.184359	7.814643	-0.041523	4.095145
201.577960	5730.174708	7.819648	-0.041553	4.097896
201.687232	5738.216932	7.824653	-0.041579	4.100664
201.595077	5746.196053	7.829658	-0.041568	4.103405
201.916341	5754.224685	7.834662	-0.041633	4.106167
202.310367	5762.250635	7.839667	-0.041712	4.108926
202.424165	5770.280012	7.844672	-0.041738	4.111682
202.627323	5778.309643	7.849677	-0.041782	4.114437
202.731996	5786.341143	7.854682	-0.041807	4.117189
202.784090	5794.319811	7.859686	-0.041822	4.119921
202.905932	5802.355998	7.864691	-0.041850	4.122671
203.273426	5810.305413	7.869696	-0.041924	4.125393
203.139713	5818.376443	7.874701	-0.041905	4.128149
203.523516	5826.396429	7.879706	-0.041982	4.130892
203.766480	5834.423361	7.884710	-0.042032	4.133633
203.954629	5842.489771	7.889715	-0.042073	4.136385
203.840669	5850.456070	7.894720	-0.042057	4.139098
204.024504	5858.497641	7.899725	-0.042097	4.141838
204.290942	5866.471929	7.904730	-0.042152	4.144555
204.322588	5874.544360	7.909734	-0.042163	4.147300
204.439401	5882.550236	7.914739	-0.042191	4.150022
204.691850	5890.584278	7.919744	-0.042243	4.152753
204.868853	5898.639227	7.924749	-0.042282	4.155488
204.869429	5906.591463	7.929754	-0.042287	4.158185
205.175044	5914.607507	7.934758	-0.042349	4.160905
205.397464	5922.620706	7.939763	-0.042396	4.163622
205.680794	5930.656547	7.944768	-0.042455	4.166345
205.862960	5938.673485	7.949773	-0.042494	4.169058
205.974396	5946.703647	7.954778	-0.042520	4.171774
206.066805	5954.743428	7.959782	-0.042543	4.174491
206.286759	5962.742629	7.964787	-0.042589	4.177193
206.536074	5970.706332	7.969792	-0.042641	4.179883
206.696830	5978.784710	7.974797	-0.042677	4.182608
206.800769	5986.719185	7.979802	-0.042702	4.185282
206.714714	5994.811498	7.984806	-0.042691	4.188006
207.071929	6002.830732	7.989811	-0.042763	4.190708
207.063086	6010.929243	7.994816	-0.042767	4.193431
207.342912	6018.993169	7.999821	-0.042825	4.196144
207.601796	6026.827809	8.004826	-0.042878	4.198777
207.853251	6034.891054	8.009830	-0.042931	4.201486
207.846840	6042.855924	8.014835	-0.042935	4.204157
208.138811	6050.878102	8.019840	-0.042995	4.206849
208.341257	6058.894321	8.024845	-0.043038	4.209536
208.325187	6066.946707	8.029850	-0.043040	4.212231
208.442748	6074.963773	8.034854	-0.043068	4.214914
208.848974	6082.984743	8.039859	-0.043149	4.217600
209.030264	6090.944847	8.044864	-0.043188	4.220261
209.025376	6099.036283	8.049869	-0.043193	4.222963
209.266113	6107.003004	8.054874	-0.043243	4.225623
209.392960	6115.061565	8.059878	-0.043272	4.228312
209.459798	6123.056783	8.064883	-0.043290	4.230976
209.463467	6131.098300	8.069888	-0.043296	4.233655
209.623610	6139.172303	8.074893	-0.043332	4.236343
209.910694	6147.078852	8.079898	-0.043390	4.238976
210.057324	6155.158865	8.084902	-0.043423	4.241663
210.163421	6163.120177	8.089907	-0.043449	4.244308
210.397136	6171.176994	8.094912	-0.043498	4.246985
210.708095	6179.186007	8.099917	-0.043561	4.249645
210.809084	6187.206937	8.104922	-0.043585	4.252305
211.022311	6195.219481	8.109926	-0.043630	4.254962
211.069862	6203.320879	8.114931	-0.043645	4.257645
211.543167	6211.256371	8.119936	-0.043738	4.260276
211.799197	6219.292531	8.124941	-0.043792	4.262935
211.773832	6227.268591	8.129946	-0.043792	4.265571
211.933239	6235.373264	8.134950	-0.043828	4.268250
212.176536	6243.379657	8.139955	-0.043878	4.270895
212.284723	6251.440096	8.144960	-0.043904	4.273555
212.453181	6259.466153	8.149965	-0.043941	4.276202
212.501403	6267.435904	8.154970	-0.043955	4.278828
212.619440	6275.466648	8.159974	-0.043983	4.281474
212.777524	6283.410290	8.164979	-0.044018	4.284089
212.851868	6291.461628	8.169984	-0.044037	4.286737
213.183756	6299.464034	8.174989	-0.044104	4.289370
213.278109	6307.509718	8.179994	-0.044127	4.292014
213.338766	6315.534599	8.184998	-0.044144	4.294648
213.654402	6323.554407	8.190003	-0.044208	4.297282
213.747562	6331.529409	8.195008	-0.044231	4.299897
214.017583	6339.565112	8.200013	-0.044287	4.302532
214.315607	6347.542244	8.205018	-0.044348	4.305146
214.459886	6355.605287	8.210022	-0.044380	4.307786
214.475656	6363.640068	8.215027	-0.044389	4.310414
214.820487	6371.664474	8.220032	-0.044458	4.313039
215.144746	6379.705864	8.225037	-0.044524	4.315668
214.931531	6387.684217	8.230042	-0.044490	4.318271
214.869424	6395.693558	8.235046	-0.044484	4.320883
215.195021	6403.689440	8.240051	-0.044550	4.323493
215.235798	6411.705261	8.245056	-0.044563	4.326105
215.446018	6419.730842	8.250061	-0.044608	4.328720
215.578487	6427.777464	8.255066	-0.044638	4.331340
215.774507	6435.788273	8.260070	-0.044680	4.333946
215.946761	6443.822758	8.265075	-0.044718	4.336559
216.096699	6451.780926	8.270080	-0.044751	4.339145
216.391514	6459.843780	8.275085	-0.044811	4.341765
216.351147	6467.794474	8.280090	-0.044809	4.344345
216.786090	6475.897022	8.285094	-0.044896	4.346975
216.949527	6483.853154	8.290099	-0.044932	4.349554
216.965090	6491.939547	8.295104	-0.044940	4.352173
216.978224	6500.016402	8.300109	-0.044948	4.354788
217.148456	6507.984935	8.305114	-0.044985	4.357366
217.502099	6515.946916	8.310118	-0.045057	4.359943
217.586414	6523.948983	8.315123	-0.045078	4.362529
217.562780	6531.901835	8.320128	-0.045079	4.365096
218.076481	6539.965201	8.325133	-0.045180	4.367702
217.936756	6547.972395	8.330138	-0.045160	4.370283
218.262359	6556.041426	8.335142	-0.045226	4.372886
218.671823	6564.065374	8.340147	-0.045307	4.375473
218.742740	6572.040321	8.345152	-0.045326	4.378041
219.050845	6580.078765	8.350157	-0.045389	4.380629
218.985614	6588.037516	8.355162	-0.045382	4.383188
219.450210	6596.080876	8.360166	-0.045474	4.385776
219.455603	6604.131427	8.365171	-0.045481	4.388361
219.541129	6612.109453	8.370176	-0.045502	4.390923
219.781356	6620.199523	8.375181	-0.045552	4.393519
219.692494	6628.195856	8.380186	-0.045541	4.396082
219.678344	6636.171206	8.385190	-0.045544	4.398638
219.893634	6644.230275	8.390195	-0.045590	4.401220
219.910109	6652.146189	8.395200	-0.045598	4.403753
220.109173	6660.267771	8.400205	-0.045641	4.406352
220.132362	6668.256377	8.405210	-0.045651	4.408906
220.464796	6676.267214	8.410214	-0.045718	4.411467
220.713706	6684.301760	8.415219	-0.045770	4.414033
220.722568	6692.319355	8.420224	-0.045777	4.416592
221.119953	6700.351348	8.425229	-0.045857	4.419155
221.232213	6708.370913	8.430234	-0.045883	4.421712
221.170839	6716.342853	8.435238	-0.045877	4.424251
221.425365	6724.397118	8.440243	-0.045930	4.426816
221.646347	6732.409539	8.445248	-0.045977	4.429367
221.840890	6740.483030	8.450253	-0.046018	4.431935
221.741792	6748.499590	8.455258	-0.046005	4.434482
222.049587	6756.514090	8.460262	-0.046068	4.437029
222.094452	6764.484787	8.465267	-0.046082	4.439559
222.053922	6772.467118	8.470272	-0.046080	4.442092
222.553810	6780.472406	8.475277	-0.046178	4.444632
222.549502	6788.532459	8.480282	-0.046183	4.447186
222.635255	6796.527950	8.485286	-0.046205	4.449719
222.672212	6804.632255	8.490291	-0.046217	4.452284
222.887618	6812.590940	8.495296	-0.046263	4.454803
222.980712	6820.659447	8.500301	-0.046285	4.457354
223.058901	6828.585543	8.505306	-0.046305	4.459859
223.204186	6836.637952	8.510310	-0.046338	4.462402
223.447181	6844.648358	8.515315	-0.046389	4.464931
223.414913	6852.665604	8.520320	-0.046388	4.467460
223.741648	6860.650616	8.525325	-0.046455	4.469979
224.104400	6868.727088	8.530330	-0.046528	4.472525
224.094756	6876.740007	8.535334	-0.046531	4.475048
224.284153	6884.764237	8.540339	-0.046572	4.477574
224.503453	6892.718301	8.545344	-0.046618	4.480076
224.432238	6900.762380	8.550349	-0.046611	4.482605
224.341830	6908.728678	8.555354	-0.046599	4.485108
224.496775	6916.783466	8.560359	-0.046634	4.487637
224.837696	6924.802234	8.565363	-0.046703	4.490155
224.775635	6932.813592	8.570368	-0.046696	4.492667
225.114150	6940.883424	8.575373	-0.046765	4.495198
225.240422	6948.874181	8.580378	-0.046794	4.497702
225.387815	6956.833354	8.585383	-0.046827	4.500195
225.486835	6964.878262	8.590387	-0.046851	4.502712
225.716849	6972.854700	8.595392	-0.046899	4.505208
225.913963	6980.964811	8.600397	-0.046941	4.507744
225.880097	6988.929544	8.605402	-0.046941	4.510232
226.202054	6996.984814	8.610407	-0.047006	4.512748
226.415438	7005.049572	8.615411	-0.047051	4.515265
226.426851	7012.974288	8.620416	-0.047059	4.517737
226.601326	7020.958238	8.625421	-0.047097	4.520226
226.614656	7028.978913	8.630426	-0.047105	4.522725
226.924801	7036.965827	8.635431	-0.047168	4.525212
226.977914	7045.020252	8.640435	-0.047183	4.527719
227.021913	7052.998906	8.645440	-0.047197	4.530201
227.077816	7061.094399	8.650445	-0.047213	4.532717
227.304785	7069.087800	8.655450	-0.047261	4.535201
227.355713	7077.077705	8.660455	-0.047276	4.537682
227.576515	7085.089119	8.665459	-0.047322	4.540169
227.702403	7093.114624	8.670464	-0.047351	4.542659
227.738577	7101.120909	8.675469	-0.047363	4.545141
227.873541	7109.143160	8.680474	-0.047394	4.547626
228.023002	7117.162728	8.685479	-0.047427	4.550110
228.194196	7125.222963	8.690483	-0.047465	4.552605
228.266382	7133.239704	8.695488	-0.047484	4.555084
228.521471	7141.252945	8.700493	-0.047537	4.557562
228.594704	7149.202720	8.705498	-0.047556	4.560018
228.738398	7157.223268	8.710503	-0.047588	4.562495
228.999965	7165.256877	8.715507	-0.047642	4.564975
229.086930	7173.287525	8.720512	-0.047664	4.567453
229.366532	7181.310744	8.725517	-0.047722	4.569926
229.340241	7189.334397	8.730522	-0.047722	4.572399
229.577157	7197.352424	8.735527	-0.047772	4.574868
229.451299	7205.424672	8.740531	-0.047754	4.577353
229.579954	7213.348282	8.745536	-0.047783	4.579790
230.003905	7221.439940	8.750541	-0.047868	4.582279
229.912353	7229.373802	8.755546	-0.047856	4.584717
230.146585	7237.462636	8.760551	-0.047905	4.587201
230.320346	7245.463500	8.765555	-0.047943	4.589657
230.528448	7253.488002	8.770560	-0.047987	4.592119
230.800805	7261.530036	8.775565	-0.048044	4.594585
230.756753	7269.538239	8.780570	-0.048041	4.597039
231.082364	7277.462572	8.785575	-0.048107	4.599467
231.089157	7285.554774	8.790579	-0.048114	4.601944
230.989645	7293.524881	8.795584	-0.048101	4.604383
231.362148	7301.599965	8.800589	-0.048176	4.606852
231.444348	7309.555021	8.805594	-0.048196	4.609284
231.441910	7317.589990	8.810599	-0.048201	4.611738
231.773794	7325.638424	8.815603	-0.048269	4.614195
231.805483	7333.653388	8.820608	-0.048280	4.616641
231.863957	7341.635770	8.825613	-0.048296	4.619076
232.039669	7349.677774	8.830618	-0.048335	4.621527
232.261639	7357.624732	8.835623	-0.048381	4.623948
232.308729	7365.730650	8.840627	-0.048396	4.626417
232.315718	7373.669523	8.845632	-0.048402	4.628833
232.686604	7381.764963	8.850637	-0.048477	4.631295
233.043624	7389.765206	8.855642	-0.048549	4.633727
232.978137	7397.767037	8.860647	-0.048542	4.636158
233.289064	7405.755246	8.865651	-0.048606	4.638584
233.602939	7413.769376	8.870656	-0.048670	4.641017
233.705087	7421.758541	8.875661	-0.048694	4.643440
233.762753	7429.821852	8.880666	-0.048710	4.645885
233.887831	7437.772148	8.885671	-0.048739	4.648294
233.890975	7445.873711	8.890675	-0.048745	4.650748
233.883870	7453.842337	8.895680	-0.048749	4.653161
234.255967	7461.936050	8.900685	-0.048824	4.655609
234.283143	7469.900818	8.905690	-0.048835	4.658018
234.300346	7477.877957	8.910695	-0.048843	4.660429
234.752124	7485.938427	8.915699	-0.048933	4.662863
234.807993	7493.931377	8.920704	-0.048949	4.665277
234.937890	7501.956747	8.925709	-0.048979	4.667698
234.962165	7509.926864	8.930714	-0.048989	4.670102
235.100186	7518.078763	8.935719	-0.049020	4.672560
235.416176	7526.124970	8.940723	-0.049084	4.674984
235.436657	7534.041280	8.945728	-0.049093	4.677368
235.500788	7542.061470	8.950733	-0.049111	4.679782
235.567157	7550.048477	8.955738	-0.049129	4.682184
235.654966	7557.987811	8.960743	-0.049150	4.684571
235.839584	7566.037783	8.965747	-0.049190	4.686990
235.938851	7574.034304	8.970752	-0.049214	4.689392
236.112182	7582.097838	8.975757	-0.049252	4.691813
236.277081	7590.078138	8.980762	-0.049288	4.694207
236.281601	7598.145877	8.985767	-0.049295	4.696626
236.488414	7606.142055	8.990771	-0.049339	4.699023
236.490822	7614.109718	8.995776	-0.049345	4.701410
236.834744	7622.169386	9.000781	-0.049414	4.703823
236.847062	7630.172476	9.005786	-0.049422	4.706218
236.973484	7638.150240	9.010791	-0.049451	4.708604
237.262262	7646.231539	9.015795	-0.049510	4.711019
237.590589	7654.255762	9.020800	-0.049577	4.713416
237.776547	7662.326967	9.025805	-0.049617	4.715827
237.790737	7670.229396	9.030810	-0.049625	4.718186
237.957336	7678.262681	9.035815	-0.049662	4.720582
238.312364	7686.300711	9.040819	-0.049733	4.722978
238.061225	7694.283106	9.045824	-0.049692	4.725358
238.241582	7702.367692	9.050829	-0.049731	4.727766
238.460079	7710.334125	9.055834	-0.049777	4.730138
238.481532	7718.391975	9.060839	-0.049787	4.732536
238.671418	7726.426160	9.065843	-0.049827	4.734925
239.028519	7734.395756	9.070848	-0.049899	4.737293
238.942357	7742.436495	9.075853	-0.049889	4.739683
239.136094	7750.448384	9.080858	-0.049930	4.742062
239.209223	7758.412626	9.085863	-0.049950	4.744426
239.611922	7766.483315	9.090867	-0.050030	4.746819
239.563683	7774.430154	9.095872	-0.050026	4.749176
239.875592	7782.549254	9.100877	-0.050090	4.751581
239.778068	7790.587895	9.105882	-0.050077	4.753963
239.874671	7798.582130	9.110887	-0.050101	4.756330
239.906580	7806.541657	9.115891	-0.050112	4.758686
240.194308	7814.511332	9.120896	-0.050171	4.761042
240.392824	7822.594907	9.125901	-0.050214	4.763431
240.193144	7830.523488	9.130906	-0.050182	4.765775
240.414380	7838.575299	9.135911	-0.050229	4.768152
240.683390	7846.638170	9.140915	-0.050284	4.770532
240.635692	7854.610118	9.145920	-0.050281	4.772884
240.890616	7862.648148	9.150925	-0.050334	4.775254
241.251393	7870.645057	9.155930	-0.050407	4.777610
241.320100	7878.652759	9.160935	-0.050425	4.779969
241.429333	7886.698934	9.165939	-0.050451	4.782337
241.398604	7894.665531	9.170944	-0.050451	4.784682
241.594602	7902.712436	9.175949	-0.050493	4.787049
241.799886	7910.733800	9.180954	-0.050536	4.789407
241.857306	7918.740085	9.185959	-0.050552	4.791759
242.095959	7926.756157	9.190963	-0.050602	4.794113
241.836971	7934.802979	9.195968	-0.050560	4.796477
242.114980	7942.779749	9.200973	-0.050617	4.798816
242.254820	7950.793573	9.205978	-0.050648	4.801166
242.453035	7958.776062	9.210983	-0.050691	4.803506
242.562696	7966.871987	9.215987	-0.050717	4.805877
242.707336	7974.794450	9.220992	-0.050749	4.808197
243.013947	7982.878055	9.225997	-0.050812	4.810562
243.034521	7990.296253	9.231002	-0.050821	4.812732
243.216316	7994.728904	9.236007	-0.050858	4.814028

243.552015	7997.241161	9.241011	-0.050922	4.814761
243.365292	7998.533337	9.246016	-0.050888	4.815140
243.522964	7998.989746	9.251021	-0.050918	4.815272
243.438381	7999.827725	9.256026	-0.050903	4.815518
243.767015	7999.807475	9.261031	-0.050965	4.815510
243.655707	7999.867622	9.266035	-0.050944	4.815528
243.728701	7999.809033	9.271040	-0.050958	4.815511
243.916988	7999.886878	9.276045	-0.050994	4.815533
243.995030	7999.905260	9.281050	-0.051008	4.815538
243.823686	7999.820262	9.286055	-0.050977	4.815514
244.075272	7999.889529	9.291059	-0.051024	4.815533
243.980932	7999.869860	9.296064	-0.051007	4.815528
244.092802	7999.894133	9.301069	-0.051028	4.815534
243.957999	7999.893026	9.306074	-0.051003	4.815534
244.135825	7999.890609	9.311079	-0.051036	4.815533
244.256037	7999.934241	9.316083	-0.051059	4.815545
244.159680	7999.884638	9.321088	-0.051041	4.815531
244.453061	7999.921482	9.326093	-0.051096	4.815540
244.256687	7999.891606	9.331098	-0.051060	4.815532
244.112266	7999.868984	9.336103	-0.051033	4.815527
244.486543	7999.914623	9.341107	-0.051103	4.815538
244.281319	7999.868583	9.346112	-0.051065	4.815526
244.477565	7999.887825	9.351117	-0.051102	4.815530
244.502462	7999.865828	9.356122	-0.051107	4.815524
244.458779	7999.886498	9.361127	-0.051099	4.815530
244.418943	7999.885871	9.366131	-0.051092	4.815530
244.277752	7999.861166	9.371136	-0.051066	4.815523
244.651479	7999.921748	9.376141	-0.051136	4.815539
244.457328	7999.878024	9.381146	-0.051100	4.815528
244.473819	7999.862298	9.386151	-0.051103	4.815523
244.668809	7999.903946	9.391155	-0.051140	4.815534
244.573391	7999.870375	9.396160	-0.051122	4.815525
244.550729	7999.895659	9.401165	-0.051118	4.815532
244.548845	7999.890312	9.406170	-0.051118	4.815531
244.545071	7999.848625	9.411175	-0.051118	4.815518
244.858047	7999.908217	9.416179	-0.051176	4.815534
244.629298	7999.876743	9.421184	-0.051134	4.815526
244.935871	7999.879631	9.426189	-0.051191	4.815526
244.661102	7999.905075	9.431194	-0.051140	4.815534
244.699179	7999.822422	9.436199	-0.051148	4.815510
244.987507	7999.858117	9.441203	-0.051202	4.815519
244.919413	7999.824992	9.446208	-0.051189	4.815510
244.922240	7999.843216	9.451213	-0.051190	4.815515
245.006634	7999.888401	9.456218	-0.051206	4.815528
245.091570	7999.875926	9.461223	-0.051222	4.815524
245.172423	7999.869793	9.466227	-0.051237	4.815522
244.885723	7999.853393	9.471232	-0.051184	4.815518
245.182558	7999.839035	9.476237	-0.051240	4.815513
245.142378	7999.869373	9.481242	-0.051233	4.815522
244.989140	7999.850878	9.486247	-0.051204	4.815517
245.188874	7999.861635	9.491251	-0.051242	4.815519
245.284177	7999.843990	9.496256	-0.051260	4.815513
245.593882	7999.865084	9.501261	-0.051318	4.815518
245.465857	7999.903601	9.506266	-0.051294	4.815530
245.238609	7999.847588	9.511271	-0.051252	4.815515
245.519748	7999.848994	9.516275	-0.051305	4.815514
245.242673	7999.799644	9.521280	-0.051253	4.815501
245.472070	7999.913407	9.526285	-0.051296	4.815533
245.346919	7999.946630	9.531290	-0.051273	4.815543
245.288237	7999.918998	9.536295	-0.051263	4.815535
245.434264	7999.929947	9.541299	-0.051290	4.815538
245.547152	7999.910453	9.546304	-0.051312	4.815532
245.380557	7999.883196	9.551309	-0.051281	4.815524
245.527932	7999.943293	9.556314	-0.051309	4.815541
245.659707	7999.871778	9.561319	-0.051333	4.815520
245.708163	7999.960163	9.566323	-0.051343	4.815545
245.532897	7999.910338	9.571328	-0.051310	4.815532
245.741557	7999.923377	9.576333	-0.051349	4.815534
245.604347	7999.928637	9.581338	-0.051324	4.815537
245.539407	7999.817603	9.586343	-0.051312	4.815504
245.602488	7999.889140	9.591347	-0.051324	4.815525
245.690508	7999.863901	9.596352	-0.051341	4.815517
245.711082	7999.886686	9.601357	-0.051345	4.815524
245.700830	7999.861980	9.606362	-0.051343	4.815517
245.783285	7999.847329	9.611367	-0.051359	4.815512
245.807680	7999.871245	9.616371	-0.051364	4.815519
245.721857	7999.873072	9.621376	-0.051348	4.815520
245.773389	7999.898499	9.626381	-0.051358	4.815527
245.655330	7999.896596	9.631386	-0.051336	4.815527
245.485018	7999.875686	9.636391	-0.051305	4.815522
245.598906	7999.929896	9.641395	-0.051326	4.815537
245.426133	7999.908946	9.646400	-0.051294	4.815532
245.479198	7999.900224	9.651405	-0.051304	4.815529
245.411493	7999.883123	9.656410	-0.051292	4.815524
245.579574	7999.865598	9.661415	-0.051324	4.815518
245.771501	7999.861277	9.666419	-0.051360	4.815516
245.649497	7999.833679	9.671424	-0.051337	4.815508
245.584797	7999.900995	9.676429	-0.051325	4.815528
245.856165	7999.902243	9.681434	-0.051376	4.815528
245.600033	7999.857505	9.686439	-0.051329	4.815516
245.643732	7999.912706	9.691443	-0.051337	4.815532
245.658823	7999.840356	9.696448	-0.051340	4.815510
246.008849	7999.898420	9.701453	-0.051406	4.815526
245.855495	7999.920504	9.706458	-0.051377	4.815533
245.578454	7999.876493	9.711463	-0.051326	4.815521
245.628066	7999.941402	9.716467	-0.051336	4.815540
245.628135	7999.857059	9.721472	-0.051336	4.815515
245.710545	7999.900077	9.726477	-0.051352	4.815528
245.717501	7999.899146	9.731482	-0.051353	4.815527
245.792497	7999.814957	9.736487	-0.051367	4.815502
245.839452	7999.868076	9.741491	-0.051376	4.815518
246.037247	7999.871327	9.746496	-0.051413	4.815518
245.893126	7999.920260	9.751501	-0.051387	4.815532
245.797105	7999.901629	9.756506	-0.051369	4.815528
245.852289	7999.901485	9.761511	-0.051380	4.815527
246.133537	7999.969107	9.766515	-0.051432	4.815546
245.887903	8000.008908	9.771520	-0.051387	4.815558
245.908702	7999.930242	9.776525	-0.051391	4.815535
245.945364	7999.899893	9.781530	-0.051398	4.815526
246.033291	7999.893876	9.786535	-0.051415	4.815524
245.854956	7999.927299	9.791539	-0.051382	4.815535
245.701512	7999.915207	9.796544	-0.051354	4.815532
245.809891	7999.896708	9.801549	-0.051374	4.815526
245.792072	7999.923140	9.806554	-0.051371	4.815534
245.914237	7999.999913	9.811559	-0.051394	4.815556
245.910684	7999.940073	9.816563	-0.051394	4.815538
245.872656	7999.924525	9.821568	-0.051387	4.815534
246.256202	7999.986341	9.826573	-0.051459	4.815550
246.200776	7999.926722	9.831578	-0.051448	4.815533
246.147924	7999.909864	9.836583	-0.051439	4.815528
246.115000	7999.962747	9.841587	-0.051433	4.815544
246.083316	7999.946234	9.846592	-0.051427	4.815539
246.273907	7999.986747	9.851597	-0.051463	4.815550
246.090794	7999.941063	9.856602	-0.051429	4.815537
245.960197	7999.905849	9.861607	-0.051405	4.815528
246.303004	7999.960593	9.866611	-0.051469	4.815542
246.031142	7999.903849	9.871616	-0.051419	4.815527
246.090084	7999.945417	9.876621	-0.051430	4.815539
246.269736	7999.930217	9.881626	-0.051464	4.815533
246.146273	7999.930361	9.886631	-0.051441	4.815534
246.107287	7999.926545	9.891635	-0.051434	4.815533
245.906299	7999.979890	9.896640	-0.051397	4.815550
246.124652	7999.925807	9.901645	-0.051438	4.815533
246.408467	7999.896287	9.906650	-0.051491	4.815523
246.317712	7999.959975	9.911655	-0.051475	4.815542
246.104876	7999.947981	9.916659	-0.051435	4.815539
246.016606	7999.930545	9.921664	-0.051419	4.815535
246.183666	7999.927955	9.926669	-0.051450	4.815533
246.303126	7999.969442	9.931674	-0.051473	4.815545
246.425437	7999.944763	9.936679	-0.051496	4.815537
246.170536	7999.922471	9.941683	-0.051449	4.815532
246.088303	7999.924356	9.946688	-0.051434	4.815532
246.250307	7999.929159	9.951693	-0.051464	4.815533
246.213585	7999.996933	9.956698	-0.051458	4.815553
246.094458	7999.918119	9.961703	-0.051436	4.815531
246.078473	7999.937104	9.966707	-0.051433	4.815536
246.003380	7999.942310	9.971712	-0.051419	4.815538
246.147312	7999.953226	9.976717	-0.051446	4.815541
246.070568	7999.943453	9.981722	-0.051432	4.815538
246.272054	7999.940357	9.986727	-0.051470	4.815536
246.258775	7999.957251	9.991731	-0.051468	4.815541
246.183505	7999.878085	9.996736	-0.051454	4.815518
246.397394	7999.961696	10.001741	-0.051494	4.815542
246.472218	7999.934106	10.006746	-0.051508	4.815533
246.339529	7999.897789	10.011751	-0.051484	4.815523
246.397116	7999.959626	10.016755	-0.051495	4.815541
246.301077	7999.938858	10.021760	-0.051477	4.815536
246.340936	7999.930989	10.026765	-0.051485	4.815533
246.298398	7999.938861	10.031770	-0.051477	4.815536
246.282364	7999.986681	10.036775	-0.051475	4.815550
246.212316	7999.927891	10.041779	-0.051462	4.815533
246.171949	7999.921916	10.046784	-0.051455	4.815531
246.335108	7999.940622	10.051789	-0.051485	4.815536
246.230967	7999.959237	10.056794	-0.051466	4.815542
246.347871	7999.952625	10.061799	-0.051488	4.815539
246.440763	7999.972320	10.066803	-0.051506	4.815545
246.338960	7999.899128	10.071808	-0.051487	4.815524
246.211844	7999.902416	10.076813	-0.051464	4.815525
246.091749	7999.905819	10.081818	-0.051441	4.815527
246.416192	7999.892983	10.086823	-0.051502	4.815522
246.387411	7999.952342	10.091827	-0.051497	4.815539
246.189635	7999.949137	10.096832	-0.051461	4.815539
246.308342	7999.988477	10.101837	-0.051483	4.815550
246.279607	7999.960264	10.106842	-0.051478	4.815542
246.287516	7999.963621	10.111847	-0.051480	4.815543
246.343318	7999.989118	10.116851	-0.051490	4.815550
246.407035	7999.953871	10.121856	-0.051502	4.815539
246.344108	7999.948595	10.126861	-0.051491	4.815538
246.373919	7999.952309	10.131866	-0.051497	4.815539
246.432377	7999.922315	10.136871	-0.051508	4.815530
246.292900	8000.036471	10.141875	-0.051482	4.815564
246.072486	7999.936779	10.146880	-0.051441	4.815536
246.370245	7999.980110	10.151885	-0.051497	4.815547
246.343264	7999.966877	10.156890	-0.051492	4.815543
246.255814	7999.909939	10.161895	-0.051476	4.815527
246.391411	7999.944214	10.166899	-0.051502	4.815537
246.549979	7999.964981	10.171904	-0.051532	4.815542
246.688622	7999.989696	10.176909	-0.051558	4.815548
246.466023	7999.982881	10.181914	-0.051517	4.815547
246.502147	8000.009126	10.186919	-0.051524	4.815555
246.632575	8000.015550	10.191923	-0.051548	4.815556
246.251529	7999.941003	10.196928	-0.051477	4.815536
246.266681	7999.948750	10.201933	-0.051480	4.815538
246.424822	7999.949218	10.206938	-0.051510	4.815538
246.385997	7999.921909	10.211943	-0.051503	4.815530
246.750367	7999.968463	10.216947	-0.051571	4.815542
246.488539	7999.911882	10.221952	-0.051523	4.815527
246.407099	7999.941547	10.226957	-0.051508	4.815536
246.431341	7999.956917	10.231962	-0.051513	4.815540
246.554349	7999.950405	10.236967	-0.051536	4.815537
246.769865	7999.988122	10.241971	-0.051576	4.815547
246.493071	7999.963335	10.246976	-0.051525	4.815542
246.698112	7999.992337	10.251981	-0.051563	4.815549
246.765118	7999.967823	10.256986	-0.051576	4.815542
246.500252	7999.918667	10.261991	-0.051527	4.815528
246.474450	7999.965260	10.266995	-0.051523	4.815542
246.504975	7999.914519	10.272000	-0.051529	4.815527
246.510262	7999.993659	10.277005	-0.051530	4.815550
246.446202	7999.983025	10.282010	-0.051518	4.815547
246.502695	7999.975427	10.287015	-0.051529	4.815545
246.781627	8000.016315	10.292019	-0.051581	4.815556
246.613977	7999.976222	10.297024	-0.051550	4.815545
246.440301	7999.995838	10.302029	-0.051518	4.815551
246.598577	7999.965338	10.307034	-0.051548	4.815542
246.438850	7999.944598	10.312039	-0.051518	4.815536
246.537745	7999.985751	10.317043	-0.051537	4.815548
246.614957	7999.957131	10.322048	-0.051552	4.815539
246.663491	8000.000666	10.327053	-0.051561	4.815552
246.492031	7999.978667	10.332058	-0.051529	4.815546
246.629985	7999.968127	10.337063	-0.051555	4.815542
246.587261	7999.984540	10.342067	-0.051548	4.815547
246.445519	7999.885064	10.347072	-0.051521	4.815519
246.732807	7999.926088	10.352077	-0.051575	4.815529
246.627644	7999.989541	10.357082	-0.051556	4.815548
246.584320	8000.019829	10.362087	-0.051548	4.815557
246.612701	7999.990412	10.367091	-0.051554	4.815549
246.596555	7999.965608	10.372096	-0.051551	4.815542
246.644246	7999.957867	10.377101	-0.051560	4.815539
246.646165	7999.966465	10.382106	-0.051561	4.815542
246.702632	7999.936439	10.387111	-0.051571	4.815532
247.005058	7999.948876	10.392115	-0.051628	4.815535
246.720720	7999.946393	10.397120	-0.051575	4.815535
246.471534	7999.953028	10.402125	-0.051529	4.815538
246.791534	7999.959343	10.407130	-0.051589	4.815539
246.807359	7999.909430	10.412135	-0.051592	4.815524
246.856081	8000.011707	10.417139	-0.051602	4.815554
246.930774	7999.999066	10.422144	-0.051616	4.815550
246.887379	8000.004789	10.427149	-0.051608	4.815552
246.849579	7999.991379	10.432154	-0.051601	4.815548
246.692826	7999.914085	10.437159	-0.051572	4.815526
246.842847	7999.959277	10.442163	-0.051601	4.815538
246.779733	7999.962542	10.447168	-0.051589	4.815540
246.701957	7999.985859	10.452173	-0.051575	4.815547
246.877033	7999.990877	10.457178	-0.051608	4.815547
246.773449	7999.992413	10.462183	-0.051589	4.815548
246.758699	8000.047730	10.467187	-0.051586	4.815565
246.850577	8000.035370	10.472192	-0.051604	4.815561
246.757079	8000.029595	10.477197	-0.051586	4.815559
246.668124	7999.990786	10.482202	-0.051570	4.815548
246.747870	7999.971820	10.487207	-0.051585	4.815542
247.005761	8000.035862	10.492211	-0.051634	4.815560
246.861022	7999.984394	10.497216	-0.051607	4.815546
246.772482	7999.976564	10.502221	-0.051591	4.815544
246.759413	8000.000938	10.507226	-0.051588	4.815551
246.879748	7999.994382	10.512231	-0.051611	4.815548
246.820216	8000.007317	10.517235	-0.051600	4.815552
246.704952	7999.970215	10.522240	-0.051579	4.815542
246.957664	7999.987180	10.527245	-0.051626	4.815546
246.796410	8000.013406	10.532250	-0.051597	4.815554
246.509946	7999.997005	10.537255	-0.051544	4.815551
246.756752	8000.017077	10.542259	-0.051590	4.815556
246.654190	7999.966299	10.547264	-0.051571	4.815541
246.691567	7999.941301	10.552269	-0.051578	4.815534
246.729095	7999.948345	10.557274	-0.051585	4.815536
246.799903	7999.885446	10.562279	-0.051599	4.815517
246.927922	7999.966590	10.567283	-0.051623	4.815540
246.923560	7999.950522	10.572288	-0.051622	4.815535
246.789457	7999.966512	10.577293	-0.051598	4.815541
246.890052	7999.986333	10.582298	-0.051617	4.815546
246.576070	7999.957735	10.587303	-0.051559	4.815539
246.928520	7999.989144	10.592307	-0.051624	4.815547
246.905851	7999.979186	10.597312	-0.051621	4.815544
246.846188	8000.014546	10.602317	-0.051610	4.815554
246.667408	7999.988155	10.607322	-0.051577	4.815547
246.793791	7999.975290	10.612327	-0.051600	4.815543
246.726180	8000.021201	10.617331	-0.051588	4.815557
246.620825	7999.974649	10.622336	-0.051569	4.815544
246.675149	8000.018278	10.627341	-0.051579	4.815556
246.746631	8000.017333	10.632346	-0.051593	4.815556
246.566541	7999.938589	10.637351	-0.051559	4.815533
246.840660	8000.022119	10.642355	-0.051611	4.815557
246.847173	7999.967781	10.647360	-0.051612	4.815541
247.082775	8000.000487	10.652365	-0.051656	4.815549
246.908841	8000.011554	10.657370	-0.051624	4.815553
246.849006	8000.028757	10.662375	-0.051613	4.815558
246.833306	8000.048815	10.667379	-0.051611	4.815564
246.762561	7999.986808	10.672384	-0.051598	4.815547
246.915291	8000.021365	10.677389	-0.051627	4.815556
247.105976	8000.012754	10.682394	-0.051662	4.815552
246.798832	7999.984267	10.687399	-0.051605	4.815546
246.968818	8000.036193	10.692403	-0.051637	4.815560
246.919424	7999.989486	10.697408	-0.051628	4.815547
247.044957	7999.964860	10.702413	-0.051652	4.815539
246.839314	7999.993565	10.707418	-0.051614	4.815548
247.103291	7999.950907	10.712423	-0.051663	4.815534
247.300510	7999.961627	10.717427	-0.051700	4.815537
247.252045	7999.986491	10.722432	-0.051692	4.815544
247.152012	8000.006241	10.727437	-0.051673	4.815550
247.245541	8000.023811	10.732442	-0.051691	4.815555
247.012332	8000.009346	10.737447	-0.051648	4.815552
247.171090	8000.042934	10.742451	-0.051678	4.815561
247.062095	7999.966418	10.747456	-0.051658	4.815539
247.175151	7999.966152	10.752461	-0.051679	4.815538
247.157785	8000.005407	10.757466	-0.051676	4.815550
247.062951	7999.962230	10.762471	-0.051659	4.815538
247.273613	8000.024433	10.767475	-0.051698	4.815555
247.084905	8000.012831	10.772480	-0.051663	4.815552
246.883543	7999.978595	10.777485	-0.051626	4.815543
247.098977	8000.032331	10.782490	-0.051666	4.815558
247.169478	8000.042050	10.787495	-0.051680	4.815561
246.770510	8000.057986	10.792499	-0.051606	4.815567
246.881104	8000.020300	10.797504	-0.051627	4.815556
246.916390	7999.986724	10.802509	-0.051633	4.815546
247.105810	7999.965276	10.807514	-0.051669	4.815538
247.087583	7999.988498	10.812519	-0.051666	4.815545
247.175588	7999.997434	10.817523	-0.051682	4.815547
247.038719	7999.980271	10.822528	-0.051657	4.815543
246.968836	8000.001581	10.827533	-0.051645	4.815550
247.114204	8000.028542	10.832538	-0.051672	4.815557
247.284358	8000.009984	10.837543	-0.051704	4.815551
247.146558	7999.997077	10.842547	-0.051678	4.815547
247.195054	7999.991485	10.847552	-0.051688	4.815546
247.122446	8000.020226	10.852557	-0.051674	4.815554
247.161860	8000.004873	10.857562	-0.051682	4.815550
247.153946	7999.948164	10.862567	-0.051681	4.815533
247.414465	8000.010113	10.867571	-0.051730	4.815550
247.099188	7999.962268	10.872576	-0.051671	4.815537
247.312889	8000.009569	10.877581	-0.051711	4.815550
247.443913	8000.018141	10.882586	-0.051736	4.815552
247.009838	8000.012143	10.887591	-0.051655	4.815552
247.087255	8000.036926	10.892595	-0.051670	4.815559
247.308258	8000.011723	10.897600	-0.051711	4.815551
247.440801	7999.997891	10.902605	-0.051736	4.815546
247.281769	7999.995317	10.907610	-0.051707	4.815546
247.171138	7999.944406	10.912615	-0.051687	4.815532
247.428199	8000.021251	10.917619	-0.051735	4.815553
247.307816	8000.017173	10.922624	-0.051713	4.815552
247.219026	8000.021086	10.927629	-0.051696	4.815554
247.304317	8000.019298	10.932634	-0.051713	4.815553
247.184547	7999.982122	10.937639	-0.051691	4.815543
247.257968	8000.033540	10.942643	-0.051705	4.815557
247.205288	7999.975031	10.947648	-0.051695	4.815541
247.060658	7999.997256	10.952653	-0.051668	4.815548
247.247844	8000.022765	10.957658	-0.051703	4.815554
247.323136	7999.996250	10.962663	-0.051718	4.815546
247.484432	8000.038424	10.967667	-0.051748	4.815558
247.126769	8000.004838	10.972672	-0.051682	4.815550
247.235166	7999.958571	10.977677	-0.051702	4.815536
247.478076	7999.998874	10.982682	-0.051748	4.815546
247.410685	7999.951873	10.987687	-0.051735	4.815533
247.281141	8000.005316	10.992691	-0.051711	4.815549
247.290446	7999.969180	10.997696	-0.051713	4.815538
247.315822	7999.997385	11.002701	-0.051718	4.815547
247.279055	7999.988264	11.007706	-0.051712	4.815544
247.258669	7999.962323	11.012711	-0.051708	4.815537
247.363731	8000.015326	11.017715	-0.051728	4.815552
247.313604	7999.991035	11.022720	-0.051719	4.815545
247.371860	7999.981329	11.027725	-0.051730	4.815542
247.481643	8000.025866	11.032730	-0.051751	4.815554
247.390719	7999.980616	11.037735	-0.051734	4.815541
247.404138	7999.952023	11.042739	-0.051737	4.815533
247.413803	8000.000264	11.047744	-0.051739	4.815547
247.332947	8000.012851	11.052749	-0.051724	4.815551
247.486960	8000.017526	11.057754	-0.051753	4.815552
247.602296	7999.994869	11.062759	-0.051775	4.815544
247.548965	8000.062374	11.067763	-0.051765	4.815564
247.291643	8000.005862	11.072768	-0.051718	4.815549
247.512485	8000.011628	11.077773	-0.051759	4.815550
247.499650	8000.006102	11.082778	-0.051757	4.815548
247.427345	7999.955816	11.087783	-0.051744	4.815534
247.474206	8000.013209	11.092787	-0.051753	4.815550
247.398350	7999.989565	11.097792	-0.051739	4.815544
247.465970	7999.984285	11.102797	-0.051752	4.815542
247.417111	8000.016619	11.107802	-0.051743	4.815552
247.143764	7999.957710	11.112807	-0.051692	4.815536
247.287790	8000.024165	11.117811	-0.051719	4.815554
247.306859	8000.005276	11.122816	-0.051723	4.815549
247.277367	7999.990934	11.127821	-0.051718	4.815545
247.272991	8000.009042	11.132826	-0.051717	4.815550
247.321922	8000.014136	11.137831	-0.051727	4.815551
247.364254	8000.033007	11.142835	-0.051735	4.815557
247.307911	8000.003274	11.147840	-0.051725	4.815548
247.590393	7999.995095	11.152845	-0.051778	4.815544
247.502501	7999.996887	11.157850	-0.051761	4.815545
247.337276	7999.960036	11.162855	-0.051731	4.815535
247.429215	8000.035253	11.167859	-0.051748	4.815557
247.365521	7999.987244	11.172864	-0.051737	4.815543
247.410372	7999.990136	11.177869	-0.051745	4.815544
247.410352	8000.006179	11.182874	-0.051746	4.815548
247.425185	7999.985084	11.187879	-0.051749	4.815542
247.393620	8000.031584	11.192883	-0.051743	4.815556
247.229350	8000.013973	11.197888	-0.051713	4.815552
247.332942	8000.030640	11.202893	-0.051732	4.815556
247.319074	8000.020825	11.207898	-0.051730	4.815553
247.209465	7999.932550	11.212903	-0.051710	4.815528
247.163941	8000.007658	11.217907	-0.051702	4.815550
247.444077	7999.966333	11.222912	-0.051754	4.815537
247.340826	7999.992438	11.227917	-0.051735	4.815545
247.216775	8000.010727	11.232922	-0.051712	4.815551
247.374419	7999.988761	11.237927	-0.051742	4.815543
247.546785	8000.019368	11.242931	-0.051774	4.815552
247.391560	8000.014720	11.247936	-0.051746	4.815551
247.388089	8000.028571	11.252941	-0.051745	4.815555
247.412121	8000.043939	11.257946	-0.051750	4.815559
247.324600	7999.992336	11.262951	-0.051734	4.815545
247.463509	8000.038417	11.267955	-0.051760	4.815557
247.367675	8000.011243	11.272960	-0.051743	4.815550
247.486166	7999.985433	11.277965	-0.051765	4.815542
247.481954	8000.008884	11.282970	-0.051764	4.815549
247.330112	8000.003223	11.287975	-0.051736	4.815548
247.437061	8000.071210	11.292979	-0.051757	4.815567
247.294597	8000.013370	11.297984	-0.051730	4.815551
247.473086	7999.971452	11.302989	-0.051764	4.815538
247.634666	7999.999747	11.307994	-0.051794	4.815545
247.385279	8000.004241	11.312999	-0.051748	4.815548
247.726932	8000.021593	11.318003	-0.051812	4.815551
247.625905	8000.033851	11.323008	-0.051793	4.815555
247.546714	8000.042192	11.328013	-0.051779	4.815558
247.602833	8000.044201	11.333018	-0.051790	4.815558
247.565872	8000.015852	11.338023	-0.051783	4.815550
247.504050	8000.054382	11.343027	-0.051772	4.815562
247.459966	8000.024849	11.348032	-0.051764	4.815553
247.643103	7999.942423	11.353037	-0.051798	4.815528
247.713357	7999.977770	11.358042	-0.051811	4.815538
247.556654	7999.968826	11.363047	-0.051782	4.815537
247.566723	8000.006394	11.368051	-0.051785	4.815547
247.652666	8000.028113	11.373056	-0.051801	4.815553
247.665864	8000.040101	11.378061	-0.051804	4.815557
247.611549	8000.037101	11.383066	-0.051794	4.815556
247.465126	8000.025120	11.388071	-0.051767	4.815553
247.620389	8000.031952	11.393075	-0.051796	4.815555
247.414555	8000.002981	11.398080	-0.051758	4.815547
247.432427	8000.019316	11.403085	-0.051762	4.815552
247.448657	8000.033489	11.408090	-0.051765	4.815556
247.443251	8000.008859	11.413095	-0.051764	4.815549
247.502293	8000.006643	11.418099	-0.051775	4.815548
247.412796	7999.988117	11.423104	-0.051759	4.815543
247.529670	7999.982573	11.428109	-0.051781	4.815541
247.395024	8000.011369	11.433114	-0.051756	4.815550
247.431904	7999.986363	11.438119	-0.051763	4.815542
247.601594	8000.003042	11.443123	-0.051795	4.815546
247.564932	8000.001399	11.448128	-0.051789	4.815546
247.534737	7999.993453	11.453133	-0.051783	4.815544
247.680483	8000.009741	11.458138	-0.051811	4.815548
247.512822	7999.935469	11.463143	-0.051780	4.815527
247.596429	7999.973170	11.468147	-0.051795	4.815537
247.408619	7999.959446	11.473152	-0.051761	4.815534
247.537393	7999.922057	11.478157	-0.051785	4.815523
247.565015	7999.989816	11.483162	-0.051790	4.815542
247.380367	7999.985755	11.488167	-0.051756	4.815542
247.628041	8000.027204	11.493171	-0.051803	4.815553
247.428476	8000.003676	11.498176	-0.051766	4.815547
247.320940	8000.011554	11.503181	-0.051746	4.815550
247.686003	8000.025017	11.508186	-0.051814	4.815552
247.493432	7999.964222	11.513191	-0.051779	4.815535
247.546651	7999.978999	11.518195	-0.051789	4.815539
247.715593	7999.977510	11.523200	-0.051821	4.815538
247.803179	7999.993916	11.528205	-0.051837	4.815542
247.798080	8000.008809	11.533210	-0.051837	4.815547
247.535275	7999.991723	11.538215	-0.051788	4.815543
247.805000	8000.005765	11.543219	-0.051838	4.815546
247.756800	7999.992184	11.548224	-0.051830	4.815542
247.785967	8000.015113	11.553229	-0.051835	4.815549
247.875832	8000.009128	11.558234	-0.051852	4.815547
247.816577	7999.950510	11.563239	-0.051842	4.815530
247.661906	8000.027040	11.568243	-0.051813	4.815553
247.592082	8000.001359	11.573248	-0.051800	4.815546
247.751402	8000.031753	11.578253	-0.051830	4.815554
247.618560	8000.016790	11.583258	-0.051806	4.815550
247.649579	7999.982076	11.588263	-0.051812	4.815540
247.791464	8000.038886	11.593267	-0.051839	4.815556
247.569912	8000.039562	11.598272	-0.051798	4.815557
247.450037	8000.024811	11.603277	-0.051775	4.815553
247.664416	8000.028336	11.608282	-0.051816	4.815553
247.599000	7999.985638	11.613287	-0.051804	4.815541
247.664353	8000.029450	11.618291	-0.051816	4.815553
247.589578	8000.033592	11.623296	-0.051803	4.815555
247.584872	8000.011110	11.628301	-0.051802	4.815548
247.599466	8000.043412	11.633306	-0.051805	4.815558
247.443342	8000.025933	11.638311	-0.051776	4.815553
247.558749	8000.050270	11.643315	-0.051798	4.815560
247.520208	7999.994127	11.648320	-0.051791	4.815544
247.524570	7999.978202	11.653325	-0.051792	4.815539
247.674370	8000.034073	11.658330	-0.051820	4.815555
247.685595	7999.995831	11.663335	-0.051822	4.815543
247.622512	7999.975600	11.668339	-0.051811	4.815538
247.572856	8000.003648	11.673344	-0.051802	4.815546
247.586305	8000.011367	11.678349	-0.051805	4.815548
247.590169	8000.047766	11.683354	-0.051806	4.815559
247.324322	7999.994319	11.688359	-0.051757	4.815545
247.615513	7999.975602	11.693363	-0.051811	4.815538
247.627121	7999.977951	11.698368	-0.051813	4.815538
247.500761	7999.997271	11.703373	-0.051790	4.815545
247.720674	8000.006226	11.708378	-0.051831	4.815546
247.699906	7999.977074	11.713383	-0.051828	4.815538
247.812764	8000.003506	11.718387	-0.051849	4.815545
247.689465	8000.008991	11.723392	-0.051826	4.815547
247.763937	7999.939742	11.728397	-0.051841	4.815527
247.806150	8000.007740	11.733402	-0.051849	4.815546
247.695119	7999.988861	11.738407	-0.051828	4.815541
247.721793	8000.012817	11.743411	-0.051834	4.815548
247.751379	8000.005847	11.748416	-0.051839	4.815546
247.812843	8000.000467	11.753421	-0.051851	4.815544
247.748015	8000.014383	11.758426	-0.051839	4.815548
247.585683	7999.996802	11.763431	-0.051809	4.815544
247.595659	8000.031165	11.768435	-0.051811	4.815554
247.662811	8000.002381	11.773440	-0.051824	4.815545
247.878144	8000.017671	11.778445	-0.051864	4.815549
247.756282	8000.046676	11.783450	-0.051842	4.815558
247.584006	8000.003300	11.788455	-0.051810	4.815546
247.602305	8000.024983	11.793459	-0.051814	4.815552
247.763231	7999.971030	11.798464	-0.051844	4.815536
247.741568	7999.995264	11.803469	-0.051840	4.815543
247.545364	8000.014510	11.808474	-0.051804	4.815549
247.819826	7999.984841	11.813479	-0.051855	4.815539
247.892686	7999.994599	11.818483	-0.051869	4.815542
247.462233	8000.001474	11.823488	-0.051789	4.815546
247.686525	8000.016910	11.828493	-0.051831	4.815549
247.846249	8000.006727	11.833498	-0.051861	4.815546
247.699717	7999.936003	11.838503	-0.051834	4.815526
247.801258	7999.999630	11.843507	-0.051854	4.815544
247.574370	8000.005559	11.848512	-0.051812	4.815547
247.573081	7999.987405	11.853517	-0.051812	4.815541
247.693996	8000.002220	11.858522	-0.051834	4.815545
247.533259	8000.000686	11.863527	-0.051805	4.815545
247.757053	8000.046018	11.868531	-0.051847	4.815557
247.773656	8000.020680	11.873536	-0.051850	4.815550
247.743562	8000.036232	11.878541	-0.051845	4.815555
247.604164	8000.038250	11.883546	-0.051819	4.815556
247.465951	8000.030675	11.888551	-0.051794	4.815554
247.644900	8000.036826	11.893555	-0.051827	4.815555
247.582632	7999.985636	11.898560	-0.051816	4.815541
247.507708	8000.010067	11.903565	-0.051802	4.815548
247.726652	8000.011531	11.908570	-0.051843	4.815547
247.663149	7999.976341	11.913575	-0.051832	4.815537
247.592686	8000.028614	11.918579	-0.051819	4.815553
247.558584	8000.021672	11.923584	-0.051813	4.815551
247.719711	8000.044620	11.928589	-0.051843	4.815557
247.644637	8000.037009	11.933594	-0.051829	4.815555
247.668927	7999.986164	11.938599	-0.051834	4.815540
247.751128	8000.014231	11.943603	-0.051850	4.815548
247.745778	7999.981058	11.948608	-0.051849	4.815538
247.697358	8000.008059	11.953613	-0.051840	4.815547
247.625330	8000.020790	11.958618	-0.051827	4.815551
247.663018	7999.989389	11.963623	-0.051834	4.815541
247.737176	8000.039752	11.968627	-0.051848	4.815556
247.806450	8000.025955	11.973632	-0.051862	4.815551
247.905154	8000.024387	11.978637	-0.051880	4.815550
247.887455	8000.024122	11.983642	-0.051877	4.815550
247.645062	8000.013777	11.988647	-0.051832	4.815548
247.856573	8000.027936	11.993651	-0.051872	4.815552
247.806667	8000.030348	11.998656	-0.051863	4.815552
247.795771	8000.017377	12.003661	-0.051861	4.815549
247.817536	8000.066885	12.008666	-0.051865	4.815563
247.707706	8000.004237	12.013671	-0.051845	4.815545
247.909812	7999.980862	12.018675	-0.051883	4.815537
247.687299	7999.994338	12.023680	-0.051842	4.815542
247.563831	7999.965644	12.028685	-0.051819	4.815535
247.708691	8000.010755	12.033690	-0.051847	4.815547
247.607985	7999.983500	12.038695	-0.051828	4.815540
247.595420	8000.020699	12.043699	-0.051826	4.815551
247.789897	8000.014287	12.048704	-0.051862	4.815548
247.772399	8000.001209	12.053709	-0.051859	4.815544
248.005527	8000.022129	12.058714	-0.051903	4.815549
247.616057	7999.996565	12.063719	-0.051831	4.815543
247.721622	8000.026082	12.068723	-0.051851	4.815552
247.770874	7999.991665	12.073728	-0.051860	4.815541
247.667279	7999.973976	12.078733	-0.051841	4.815537
247.783280	8000.015411	12.083738	-0.051863	4.815548
247.731341	7999.939825	12.088743	-0.051854	4.815526
247.627608	7999.999030	12.093747	-0.051835	4.815544
247.643104	8000.005715	12.098752	-0.051838	4.815546
247.777114	8000.021812	12.103757	-0.051863	4.815550
247.755661	8000.038573	12.108762	-0.051859	4.815555
247.566567	7999.965018	12.113767	-0.051824	4.815534
247.665616	8000.014720	12.118771	-0.051843	4.815548
247.617401	8000.005412	12.123776	-0.051834	4.815546
247.688041	7999.953188	12.128781	-0.051848	4.815530
247.964247	7999.956656	12.133786	-0.051899	4.815530
247.858830	7999.995542	12.138791	-0.051880	4.815542
247.779209	7999.999605	12.143795	-0.051866	4.815543
247.835377	7999.995206	12.148800	-0.051876	4.815542
247.828291	7999.889380	12.153805	-0.051875	4.815511
247.843438	7999.935575	12.158810	-0.051878	4.815524
247.753458	7999.897816	12.163815	-0.051862	4.815514
247.884763	7999.968338	12.168819	-0.051886	4.815534
247.837802	8000.019927	12.173824	-0.051878	4.815549
247.857190	7999.992498	12.178829	-0.051882	4.815541
248.077852	8000.027100	12.183834	-0.051923	4.815550
247.741007	7999.995987	12.188839	-0.051861	4.815542
247.692474	7999.980265	12.193843	-0.051852	4.815538
247.809400	7999.982199	12.198848	-0.051874	4.815538
247.937018	7999.975763	12.203853	-0.051898	4.815536
247.892101	7999.952624	12.208858	-0.051890	4.815529
247.771897	7999.934664	12.213863	-0.051868	4.815524
248.076767	8000.019770	12.218867	-0.051925	4.815548
247.805994	7999.981192	12.223872	-0.051875	4.815538
247.783770	7999.963764	12.228877	-0.051871	4.815533
247.886461	8000.035955	12.233882	-0.051890	4.815553
247.732852	7999.966183	12.238887	-0.051862	4.815534
247.859561	7999.987501	12.243891	-0.051886	4.815539
247.919599	7999.977825	12.248896	-0.051897	4.815536
247.874307	8000.001673	12.253901	-0.051889	4.815543
248.009193	8000.022057	12.258906	-0.051914	4.815549
247.894905	8000.012736	12.263911	-0.051893	4.815547
248.028755	8000.037375	12.268915	-0.051919	4.815553
247.945017	8000.005058	12.273920	-0.051903	4.815544
247.839719	8000.009769	12.278925	-0.051884	4.815546
248.134106	7999.961201	12.283930	-0.051939	4.815530
248.025844	7999.951979	12.288935	-0.051919	4.815528
247.877045	7999.990156	12.293939	-0.051892	4.815540
247.808808	7999.997609	12.298944	-0.051879	4.815542
247.951819	7999.987153	12.303949	-0.051906	4.815539
248.024723	8000.043905	12.308954	-0.051920	4.815555
247.909931	7999.991855	12.313959	-0.051899	4.815540
247.932346	8000.020014	12.318963	-0.051903	4.815548
247.694694	8000.009746	12.323968	-0.051859	4.815547
247.785517	7999.954648	12.328973	-0.051877	4.815530
247.888578	7999.965967	12.333978	-0.051896	4.815533
247.936984	8000.008435	12.338983	-0.051905	4.815545
247.960855	7999.957583	12.343987	-0.051910	4.815530
247.685009	7999.991548	12.348992	-0.051859	4.815541
247.889747	8000.032297	12.353997	-0.051897	4.815552
247.973687	8000.049713	12.359002	-0.051913	4.815557
247.767513	7999.990830	12.364007	-0.051875	4.815541
247.957809	8000.018527	12.369011	-0.051911	4.815548
248.191244	8000.011685	12.374016	-0.051954	4.815545
247.950070	7999.989611	12.379021	-0.051910	4.815539
247.909531	8000.032761	12.384026	-0.051903	4.815552
247.821530	7999.960857	12.389031	-0.051886	4.815532
247.901598	7999.999569	12.394035	-0.051902	4.815542
247.978866	8000.022216	12.399040	-0.051916	4.815549
247.966020	7999.997465	12.404045	-0.051914	4.815542
248.118031	8000.020265	12.409050	-0.051943	4.815547
247.726320	7999.976507	12.414055	-0.051870	4.815537
247.991105	7999.994741	12.419059	-0.051920	4.815541
248.037861	8000.014753	12.424064	-0.051929	4.815546
247.950249	7999.958875	12.429069	-0.051913	4.815530
247.893157	8000.008163	12.434074	-0.051902	4.815545
247.872475	7999.976876	12.439079	-0.051899	4.815536
247.964002	8000.020047	12.444083	-0.051916	4.815548
247.710703	8000.019136	12.449088	-0.051869	4.815549
247.876553	7999.957788	12.454093	-0.051900	4.815530
248.094229	7999.999817	12.459098	-0.051941	4.815542
247.986244	8000.008756	12.464103	-0.051921	4.815545
248.059332	8000.043083	12.469107	-0.051935	4.815554
248.005515	8000.025138	12.474112	-0.051925	4.815549
248.122407	7999.999303	12.479117	-0.051947	4.815541
247.956785	8000.038273	12.484122	-0.051917	4.815553
247.877022	8000.023109	12.489127	-0.051902	4.815549
247.976082	8000.077084	12.494131	-0.051921	4.815565
247.901105	8000.041705	12.499136	-0.051907	4.815555
247.762287	8000.050141	12.504141	-0.051882	4.815558
248.017869	8000.070361	12.509146	-0.051929	4.815562
247.812749	7999.994407	12.514151	-0.051891	4.815541
247.880665	8000.009424	12.519155	-0.051904	4.815545
247.843820	8000.022730	12.524160	-0.051898	4.815549
247.982119	7999.981224	12.529165	-0.051924	4.815537
247.989471	8000.009136	12.534170	-0.051925	4.815545
247.996894	7999.994328	12.539175	-0.051927	4.815540
248.220034	8000.047128	12.544179	-0.051969	4.815555
247.940845	8000.018024	12.549184	-0.051917	4.815547
247.816974	8000.007479	12.554189	-0.051894	4.815545
248.056501	8000.048798	12.559194	-0.051939	4.815556
247.955739	8000.007657	12.564199	-0.051921	4.815544
247.921476	8000.046638	12.569203	-0.051915	4.815556
247.922391	8000.057356	12.574208	-0.051915	4.815559
247.965513	8000.037792	12.579213	-0.051923	4.815553
248.097888	8000.057067	12.584218	-0.051948	4.815558
247.922263	7999.990139	12.589223	-0.051916	4.815539
248.035446	7999.990944	12.594227	-0.051937	4.815539
247.925886	8000.023354	12.599232	-0.051917	4.815549
247.888883	8000.036657	12.604237	-0.051910	4.815553
248.001577	8000.050270	12.609242	-0.051932	4.815557
247.836109	8000.015549	12.614247	-0.051901	4.815547
247.881016	8000.039802	12.619251	-0.051910	4.815554
247.942472	8000.014129	12.624256	-0.051922	4.815546
248.042920	8000.000842	12.629261	-0.051940	4.815542
247.962978	8000.036940	12.634266	-0.051926	4.815553
247.873592	7999.971421	12.639271	-0.051909	4.815534
248.254474	8000.001165	12.644275	-0.051981	4.815541
248.161028	8000.040246	12.649280	-0.051964	4.815553
248.060932	8000.018341	12.654285	-0.051945	4.815547
247.967000	8000.039258	12.659290	-0.051928	4.815553
247.889336	7999.978203	12.664295	-0.051914	4.815536
247.878968	7999.979125	12.669299	-0.051912	4.815536
247.781335	8000.009594	12.674304	-0.051894	4.815546
247.995219	7999.982140	12.679309	-0.051934	4.815537
248.119196	8000.050407	12.684314	-0.051958	4.815556
248.017786	7999.984691	12.689319	-0.051939	4.815537
248.164955	8000.036249	12.694323	-0.051967	4.815552
248.137585	8000.021941	12.699328	-0.051962	4.815547
248.078390	7999.991092	12.704333	-0.051951	4.815539
248.250094	8000.023826	12.709338	-0.051983	4.815547
248.112499	7999.989560	12.714343	-0.051958	4.815538
248.014338	8000.013612	12.719347	-0.051940	4.815546
248.303860	8000.000210	12.724352	-0.051994	4.815540
248.241499	8000.005622	12.729357	-0.051983	4.815542
248.220974	8000.034147	12.734362	-0.051979	4.815551
247.987297	8000.026080	12.739367	-0.051936	4.815549
248.049105	8000.034590	12.744371	-0.051948	4.815552
248.147326	8000.036218	12.749376	-0.051966	4.815552
247.968468	8000.032251	12.754381	-0.051933	4.815551
248.036410	8000.039792	12.759386	-0.051946	4.815553
248.237360	8000.009991	12.764391	-0.051984	4.815543
248.060324	8000.009257	12.769395	-0.051951	4.815544
248.050057	8000.033677	12.774400	-0.051950	4.815551
248.123594	8000.022086	12.779405	-0.051963	4.815547
248.303550	8000.017574	12.784410	-0.051997	4.815545
248.000634	8000.000899	12.789415	-0.051941	4.815542
248.299329	8000.038913	12.794419	-0.051997	4.815552
248.425181	8000.028176	12.799424	-0.052021	4.815548
248.296620	7999.972697	12.804429	-0.051997	4.815532
248.283296	8000.032313	12.809434	-0.051995	4.815550
248.198195	7999.932686	12.814439	-0.051979	4.815521
248.114035	8000.013573	12.819443	-0.051964	4.815545
248.216878	8000.027025	12.824448	-0.051983	4.815548
248.154386	8000.017483	12.829453	-0.051972	4.815546
248.176060	8000.025337	12.834458	-0.051976	4.815548
248.041834	7999.979377	12.839463	-0.051951	4.815535
248.031219	7999.983499	12.844467	-0.051950	4.815537
248.104022	8000.016753	12.849472	-0.051964	4.815546
248.121696	8000.022406	12.854477	-0.051967	4.815547
247.975995	8000.028593	12.859482	-0.051940	4.815550
248.010371	8000.000341	12.864487	-0.051947	4.815542
248.036376	8000.043510	12.869491	-0.051952	4.815554
248.084760	8000.055005	12.874496	-0.051961	4.815557
247.952902	8000.013356	12.879501	-0.051937	4.815546
248.269755	8000.020694	12.884506	-0.051996	4.815546
248.084871	7999.964294	12.889511	-0.051962	4.815531
248.112990	8000.002158	12.894515	-0.051968	4.815542
248.166931	8000.005199	12.899520	-0.051978	4.815542
248.061326	8000.007769	12.904525	-0.051959	4.815543
248.118917	8000.068543	12.909530	-0.051970	4.815561
248.039606	8000.036297	12.914535	-0.051955	4.815552
248.002959	8000.022906	12.919539	-0.051948	4.815548
248.071810	8000.025122	12.924544	-0.051962	4.815548
248.089245	8000.009410	12.929549	-0.051965	4.815544
248.323682	8000.015401	12.934554	-0.052009	4.815544
248.128106	7999.944942	12.939559	-0.051973	4.815525
248.187886	7999.956622	12.944563	-0.051984	4.815528
248.172447	7999.999115	12.949568	-0.051982	4.815540
248.272663	7999.999708	12.954573	-0.052001	4.815540
248.306287	8000.073976	12.959578	-0.052007	4.815562
248.328516	8000.006008	12.964583	-0.052012	4.815542
248.389010	8000.023040	12.969587	-0.052023	4.815546
248.366678	8000.029107	12.974592	-0.052019	4.815548
248.249120	8000.033617	12.979597	-0.051998	4.815550
248.397837	8000.001894	12.984602	-0.052025	4.815540
247.947557	7999.999899	12.989607	-0.051942	4.815542
248.127962	8000.039184	12.994611	-0.051976	4.815552
248.311308	8000.031523	12.999616	-0.052010	4.815549
248.054424	8000.029484	13.004621	-0.051963	4.815550
248.080231	8000.069447	13.009626	-0.051968	4.815561
247.998042	8000.013657	13.014631	-0.051953	4.815545
248.197245	8000.011596	13.019635	-0.051990	4.815544
248.213804	8000.021502	13.024640	-0.051993	4.815547
248.224090	7999.967224	13.029645	-0.051995	4.815531
248.193734	8000.027629	13.034650	-0.051990	4.815548
248.151997	8000.008814	13.039655	-0.051983	4.815543
248.063865	8000.026622	13.044659	-0.051966	4.815549
248.186749	8000.032925	13.049664	-0.051990	4.815550
248.234209	7999.994207	13.054669	-0.051999	4.815538
248.249802	8000.032935	13.059674	-0.052002	4.815550
248.301794	7999.979338	13.064679	-0.052012	4.815534
248.275760	8000.017385	13.069683	-0.052007	4.815545
248.070199	8000.015117	13.074688	-0.051969	4.815545
248.082226	7999.980092	13.079693	-0.051972	4.815535
248.274827	8000.022780	13.084698	-0.052008	4.815547
248.104707	7999.999731	13.089703	-0.051976	4.815541
248.295404	8000.032776	13.094707	-0.052012	4.815549
248.282173	8000.028311	13.099712	-0.052010	4.815548
248.357476	8000.006068	13.104717	-0.052024	4.815541
248.489147	8000.046693	13.109722	-0.052049	4.815552
248.314341	8000.015022	13.114727	-0.052017	4.815544
248.170867	8000.043674	13.119731	-0.051990	4.815553
248.242870	7999.991472	13.124736	-0.052004	4.815537
248.224186	7999.980510	13.129741	-0.052001	4.815534
248.413299	7999.979351	13.134746	-0.052036	4.815533
248.281528	7999.965473	13.139751	-0.052012	4.815530
248.272552	7999.995255	13.144755	-0.052011	4.815538
248.395301	8000.032530	13.149760	-0.052034	4.815549
248.292500	8000.020192	13.154765	-0.052015	4.815546
248.196880	8000.059239	13.159770	-0.051997	4.815557
248.004163	8000.002711	13.164775	-0.051962	4.815542
248.159161	8000.003131	13.169779	-0.051991	4.815541
248.292845	7999.992523	13.174784	-0.052016	4.815537
248.147975	7999.963478	13.179789	-0.051989	4.815530
248.169025	8000.030063	13.184794	-0.051994	4.815549
248.214362	8000.021215	13.189799	-0.052002	4.815546
248.296050	8000.016165	13.194803	-0.052018	4.815544
248.274724	8000.019044	13.199808	-0.052014	4.815545
248.147492	7999.965723	13.204813	-0.051991	4.815530
248.290578	7999.993717	13.209818	-0.052017	4.815538
248.291628	8000.003370	13.214823	-0.052018	4.815541
248.120007	8000.004861	13.219827	-0.051986	4.815542
248.167448	8000.023816	13.224832	-0.051995	4.815547
248.340394	8000.001033	13.229837	-0.052028	4.815540
248.434368	8000.026089	13.234842	-0.052046	4.815547
248.316892	8000.007104	13.239847	-0.052024	4.815542
248.260276	8000.010474	13.244851	-0.052014	4.815543
248.175775	8000.039022	13.249856	-0.051998	4.815552
248.279265	8000.024716	13.254861	-0.052018	4.815547
248.205359	8000.020327	13.259866	-0.052004	4.815546
248.024973	8000.010995	13.264871	-0.051971	4.815544
248.209435	8000.051414	13.269875	-0.052006	4.815555
248.165524	8000.032563	13.274880	-0.051998	4.815550
248.156215	8000.022822	13.279885	-0.051996	4.815547
248.253722	8000.049004	13.284890	-0.052015	4.815554
248.263922	8000.041718	13.289895	-0.052017	4.815552
248.281761	8000.067666	13.294899	-0.052020	4.815559
248.098628	8000.027315	13.299904	-0.051987	4.815548
248.236130	7999.989000	13.304909	-0.052012	4.815537
248.124152	8000.008554	13.309914	-0.051992	4.815543
248.091064	7999.988812	13.314919	-0.051986	4.815537
248.306898	8000.003043	13.319923	-0.052026	4.815540
248.360218	8000.018890	13.324928	-0.052037	4.815545
248.260290	7999.941450	13.329933	-0.052018	4.815523
248.413222	8000.008055	13.334938	-0.052047	4.815541
248.446824	8000.006491	13.339943	-0.052054	4.815541
248.477166	8000.008079	13.344947	-0.052059	4.815541
248.241655	8000.014933	13.349952	-0.052016	4.815544
248.378370	7999.954177	13.354957	-0.052042	4.815526
248.519211	8000.002428	13.359962	-0.052068	4.815539
248.326026	7999.967253	13.364967	-0.052032	4.815530
248.290629	8000.030780	13.369971	-0.052026	4.815548
248.386871	8000.021696	13.374976	-0.052044	4.815545
248.330711	7999.984488	13.379981	-0.052034	4.815535
248.421534	8000.011629	13.384986	-0.052051	4.815542
248.144770	8000.015673	13.389991	-0.052000	4.815545
248.128616	7999.993004	13.394995	-0.051997	4.815538
248.145190	8000.028543	13.400000	-0.052001	4.815548
248.118112	8000.020648	13.405005	-0.051996	4.815546
248.227539	8000.017119	13.410010	-0.052016	4.815545
248.270672	7999.979398	13.415015	-0.052025	4.815533
248.207117	7999.944206	13.420019	-0.052013	4.815523
248.298550	7999.976697	13.425024	-0.052030	4.815532
248.327787	7999.964381	13.430029	-0.052036	4.815529
248.405190	8000.030820	13.435034	-0.052051	4.815548
248.418321	8000.002221	13.440039	-0.052054	4.815539
248.168948	8000.002441	13.445043	-0.052007	4.815541
248.298160	8000.012053	13.450048	-0.052032	4.815543
248.401501	7999.980656	13.455053	-0.052051	4.815533
248.449818	8000.033803	13.460058	-0.052060	4.815548
248.251963	8000.023116	13.465063	-0.052024	4.815546
248.282530	8000.012959	13.470067	-0.052030	4.815543
248.438957	8000.031559	13.475072	-0.052059	4.815548
248.259911	7999.998751	13.480077	-0.052026	4.815539
248.459047	8000.053296	13.485082	-0.052064	4.815554
248.289600	8000.009964	13.490087	-0.052032	4.815542
248.106846	7999.981367	13.495091	-0.051998	4.815535
248.197429	8000.002096	13.500096	-0.052016	4.815540
248.065878	8000.007446	13.505101	-0.051991	4.815542
248.256983	8000.066130	13.510106	-0.052027	4.815559
248.210654	8000.064329	13.515111	-0.052019	4.815558
248.232018	8000.063633	13.520115	-0.052023	4.815558
248.159193	8000.064602	13.525120	-0.052010	4.815559
248.146961	8000.021704	13.530125	-0.052008	4.815546
248.309283	8000.062830	13.535130	-0.052038	4.815557
248.302578	8000.034975	13.540135	-0.052037	4.815549
248.265725	8000.035464	13.545139	-0.052031	4.815550
248.453046	8000.030005	13.550144	-0.052066	4.815547
248.469148	7999.990773	13.555149	-0.052069	4.815536
248.485318	8000.014558	13.560154	-0.052072	4.815542
248.385229	7999.975564	13.565159	-0.052054	4.815532
248.228252	8000.007199	13.570163	-0.052025	4.815542
248.273527	8000.031459	13.575168	-0.052034	4.815548
248.238885	7999.983923	13.580173	-0.052028	4.815535
248.280634	8000.034827	13.585178	-0.052036	4.815549
248.229803	8000.016930	13.590183	-0.052026	4.815544
248.281057	7999.986818	13.595187	-0.052036	4.815535
248.288885	8000.036100	13.600192	-0.052038	4.815550
248.188636	8000.028076	13.605197	-0.052020	4.815548
248.365845	8000.067310	13.610202	-0.052053	4.815558
248.341016	8000.038090	13.615207	-0.052048	4.815550
248.373057	8000.003392	13.620211	-0.052055	4.815540
248.508227	8000.032326	13.625216	-0.052080	4.815547
248.436281	7999.991655	13.630221	-0.052067	4.815536
248.345052	8000.056406	13.635226	-0.052050	4.815555
248.347580	8000.025498	13.640231	-0.052051	4.815546
248.379782	8000.057021	13.645235	-0.052057	4.815555
248.310673	8000.059119	13.650240	-0.052045	4.815556
248.199421	8000.013534	13.655245	-0.052024	4.815543
248.359108	7999.999078	13.660250	-0.052054	4.815538
248.332610	7999.982648	13.665255	-0.052050	4.815534
248.270286	8000.022239	13.670259	-0.052038	4.815546
248.381393	8000.032622	13.675264	-0.052059	4.815548
248.278868	7999.963683	13.680269	-0.052040	4.815528
248.476402	7999.996840	13.685274	-0.052077	4.815537
248.442217	7999.990965	13.690279	-0.052071	4.815536
248.643647	7999.959035	13.695283	-0.052109	4.815525
248.663510	8000.035215	13.700288	-0.052113	4.815547
248.479292	8000.020478	13.705293	-0.052079	4.815544
248.482696	8000.023761	13.710298	-0.052080	4.815545
248.480442	8000.019476	13.715303	-0.052080	4.815544
248.158332	8000.030255	13.720307	-0.052020	4.815548
248.375674	8000.025286	13.725312	-0.052061	4.815546
248.208907	7999.972386	13.730317	-0.052030	4.815531
248.391905	8000.041619	13.735322	-0.052064	4.815551
248.149639	7999.950104	13.740327	-0.052019	4.815525
248.239324	7999.987906	13.745331	-0.052036	4.815536
248.191083	8000.015978	13.750336	-0.052028	4.815544
248.333061	7999.986281	13.755341	-0.052054	4.815535
248.539749	8000.023860	13.760346	-0.052093	4.815545
248.457126	8000.024669	13.765351	-0.052078	4.815545
248.295730	8000.024190	13.770355	-0.052048	4.815546
248.459844	8000.017284	13.775360	-0.052079	4.815543
248.404125	7999.966198	13.780365	-0.052069	4.815528
248.430410	8000.026462	13.785370	-0.052074	4.815546
248.375841	8000.006368	13.790375	-0.052064	4.815540
248.611453	7999.998495	13.795379	-0.052108	4.815537
248.381100	8000.043883	13.800384	-0.052066	4.815551
248.240544	8000.017044	13.805389	-0.052040	4.815544
248.268042	8000.000428	13.810394	-0.052045	4.815539
248.325453	8000.022751	13.815399	-0.052056	4.815545
248.295729	7999.962478	13.820403	-0.052051	4.815528
248.316857	8000.021589	13.825408	-0.052055	4.815545
248.142194	8000.009145	13.830413	-0.052023	4.815542
248.201700	7999.986644	13.835418	-0.052034	4.815535
248.192937	7999.940599	13.840423	-0.052033	4.815522
248.282896	7999.937820	13.845427	-0.052050	4.815521
248.311367	7999.979962	13.850432	-0.052055	4.815533
248.349354	7999.982743	13.855437	-0.052063	4.815533
248.661630	8000.010299	13.860442	-0.052121	4.815540
248.479467	7999.984916	13.865447	-0.052088	4.815533
248.312801	8000.000372	13.870451	-0.052057	4.815539
248.651132	8000.009130	13.875456	-0.052120	4.815540
248.416796	7999.964737	13.880461	-0.052077	4.815528
248.418007	8000.003230	13.885466	-0.052077	4.815539
248.237850	7999.988560	13.890471	-0.052044	4.815536
248.351430	7999.928493	13.895475	-0.052065	4.815518
248.395596	7999.999730	13.900480	-0.052074	4.815538
248.188643	7999.893839	13.905485	-0.052035	4.815508
248.334779	7999.956061	13.910490	-0.052063	4.815526
248.455496	7999.982622	13.915495	-0.052086	4.815533
248.468792	7999.974318	13.920499	-0.052088	4.815530
248.413773	8000.030049	13.925504	-0.052079	4.815547
248.411765	7999.947800	13.930509	-0.052078	4.815523
248.433949	7999.937506	13.935514	-0.052083	4.815520
248.200769	7999.944398	13.940519	-0.052040	4.815523
248.412075	7999.950011	13.945523	-0.052079	4.815523
248.509964	7999.979404	13.950528	-0.052098	4.815532
248.356325	7999.925650	13.955533	-0.052069	4.815517
248.486099	8000.014306	13.960538	-0.052094	4.815542
248.534779	7999.993764	13.965543	-0.052103	4.815536
248.273625	7999.961750	13.970547	-0.052055	4.815528
248.317421	8000.004143	13.975552	-0.052063	4.815540
248.356336	7999.988782	13.980557	-0.052071	4.815535
248.420390	8000.036846	13.985562	-0.052083	4.815549
248.197606	7999.977690	13.990567	-0.052042	4.815532
248.332634	7999.927586	13.995571	-0.052067	4.815517
248.682926	8000.014507	14.000576	-0.052133	4.815541
248.365351	7999.942052	14.005581	-0.052074	4.815521
248.333131	7999.981066	14.010586	-0.052068	4.815533
248.529947	7999.965082	14.015591	-0.052105	4.815527
248.510417	7999.948765	14.020595	-0.052102	4.815523
248.421171	7999.985780	14.025600	-0.052085	4.815534
248.427610	7999.945323	14.030605	-0.052087	4.815522
248.707042	7999.992636	14.035610	-0.052139	4.815534
248.379764	7999.983037	14.040615	-0.052078	4.815533
248.331639	7999.978002	14.045619	-0.052070	4.815532
248.543768	8000.017806	14.050624	-0.052109	4.815542
248.343791	7999.939797	14.055629	-0.052072	4.815521
248.484399	7999.979501	14.060634	-0.052099	4.815532
248.529815	7999.955701	14.065639	-0.052108	4.815524
248.516120	7999.934140	14.070643	-0.052105	4.815518
248.516051	8000.016402	14.075648	-0.052106	4.815542
248.481706	7999.996639	14.080653	-0.052099	4.815537
248.533061	8000.004978	14.085658	-0.052109	4.815539
248.377581	7999.990712	14.090663	-0.052081	4.815535
248.371772	8000.014137	14.095667	-0.052080	4.815542
248.604787	8000.014765	14.100672	-0.052123	4.815541
248.451691	7999.970632	14.105677	-0.052095	4.815529
248.440564	8000.001447	14.110682	-0.052093	4.815538
248.499988	7999.972536	14.115687	-0.052105	4.815529
248.501229	7999.950151	14.120691	-0.052105	4.815523
248.355838	7999.934982	14.125696	-0.052078	4.815519
248.344190	7999.949767	14.130701	-0.052076	4.815523
248.614559	7999.929645	14.135706	-0.052127	4.815516
248.336811	7999.908040	14.140711	-0.052076	4.815511
248.352430	7999.984150	14.145715	-0.052079	4.815533
248.526503	8000.043625	14.150720	-0.052112	4.815550
248.310408	7999.982441	14.155725	-0.052072	4.815533
248.414463	7999.963873	14.160730	-0.052091	4.815527
248.434780	7999.978113	14.165735	-0.052095	4.815531
248.511186	7999.887533	14.170739	-0.052110	4.815504
248.360849	7999.938502	14.175744	-0.052082	4.815520
248.348419	7999.914825	14.180749	-0.052080	4.815513
248.564096	7999.944006	14.185754	-0.052120	4.815521
248.543129	7999.934075	14.190759	-0.052117	4.815518
248.430062	7999.927978	14.195763	-0.052096	4.815517
248.655653	7999.984023	14.200768	-0.052138	4.815532
248.731154	7999.905177	14.205773	-0.052152	4.815508
248.511829	7999.943269	14.210778	-0.052112	4.815521
248.441927	7999.925061	14.215783	-0.052099	4.815516
248.497212	7999.993275	14.220787	-0.052110	4.815535
248.697306	8000.013659	14.225792	-0.052147	4.815540
248.392916	7999.991617	14.230797	-0.052091	4.815535
248.528842	7999.999203	14.235802	-0.052116	4.815537
248.549464	7999.716532	14.240807	-0.052120	4.815454

248.450820	7996.442817	14.245811	-0.052100	4.814498
248.398192	7990.830488	14.250816	-0.052087	4.812857
248.450286	7983.950911	14.255821	-0.052092	4.810844
248.447409	7976.669113	14.260826	-0.052087	4.808713
248.519980	7969.081507	14.265831	-0.052096	4.806491
248.518015	7961.187237	14.270835	-0.052091	4.804178
248.340561	7953.394216	14.275840	-0.052053	4.801895
248.069727	7945.356610	14.280845	-0.051998	4.799540
248.245139	7937.473315	14.285850	-0.052026	4.797226
248.162464	7929.390057	14.290855	-0.052005	4.794854
248.173042	7921.430171	14.295859	-0.052002	4.792517
248.189574	7913.378640	14.300864	-0.052000	4.790151
248.082654	7905.418551	14.305869	-0.051975	4.787812
247.925917	7897.372557	14.310874	-0.051941	4.785446
247.808341	7889.440409	14.315879	-0.051915	4.783113
248.043279	7881.436352	14.320883	-0.051953	4.780756
247.997693	7873.445153	14.325888	-0.051940	4.778403
247.896272	7865.380919	14.330893	-0.051916	4.776027
248.003916	7857.406021	14.335898	-0.051931	4.773675
247.847049	7849.374517	14.340903	-0.051897	4.771307
247.722974	7841.315749	14.345907	-0.051869	4.768929
247.790298	7833.408241	14.350912	-0.051877	4.766594
247.844191	7825.311065	14.355917	-0.051882	4.764202
247.754049	7817.474969	14.360922	-0.051860	4.761886
247.642703	7809.387028	14.365927	-0.051834	4.759495
247.740212	7801.425887	14.370931	-0.051847	4.757140
247.624047	7793.405073	14.375936	-0.051821	4.754766
247.542817	7785.283309	14.380941	-0.051801	4.752361
247.443421	7777.306659	14.385946	-0.051777	4.749998
247.455510	7769.326800	14.390951	-0.051775	4.747633
247.298707	7761.299675	14.395955	-0.051740	4.745252
247.382837	7753.388538	14.400960	-0.051751	4.742905
247.246674	7745.347634	14.405965	-0.051721	4.740518
247.284976	7737.386139	14.410970	-0.051723	4.738153
247.166130	7729.285285	14.415975	-0.051696	4.735746
247.327567	7721.360304	14.420979	-0.051721	4.733389
247.461891	7713.315152	14.425984	-0.051741	4.730996
247.177035	7705.294287	14.430989	-0.051683	4.728609
247.310882	7697.332724	14.435994	-0.051703	4.726238
247.252399	7689.306368	14.440999	-0.051687	4.723847
247.118521	7681.308585	14.446003	-0.051657	4.721463
247.170571	7673.348914	14.451008	-0.051662	4.719089
247.027953	7665.318408	14.456013	-0.051631	4.716693
246.906140	7657.339260	14.461018	-0.051603	4.714312
246.752417	7649.300205	14.466023	-0.051569	4.711911
247.002040	7641.247517	14.471027	-0.051611	4.709504
246.863208	7633.325401	14.476032	-0.051580	4.707135
246.568305	7625.263256	14.481037	-0.051520	4.704724
246.720348	7617.357655	14.486042	-0.051544	4.702358
246.716530	7609.319409	14.491047	-0.051538	4.699951
246.725225	7601.351007	14.496051	-0.051535	4.697563
246.515434	7593.275910	14.501056	-0.051491	4.695143
246.633285	7585.266451	14.506061	-0.051508	4.692741
246.671163	7577.268889	14.511066	-0.051510	4.690341
246.368792	7569.274439	14.516071	-0.051449	4.687941
246.430135	7561.264469	14.521075	-0.051455	4.685535
246.518090	7553.315865	14.526080	-0.051466	4.683146
246.545240	7545.299343	14.531085	-0.051467	4.680736
246.367003	7537.280703	14.536090	-0.051428	4.678324
246.473681	7529.312276	14.541095	-0.051443	4.675925
246.406679	7521.219598	14.546099	-0.051426	4.673488
246.044114	7513.140187	14.551104	-0.051353	4.671054
245.947084	7505.168792	14.556109	-0.051330	4.668651
246.002411	7497.208391	14.561114	-0.051336	4.666250
246.028004	7489.187832	14.566119	-0.051336	4.663829
246.261322	7481.302471	14.571123	-0.051374	4.661448
246.024542	7473.280918	14.576128	-0.051325	4.659025
246.001241	7465.225124	14.581133	-0.051316	4.656590
246.034964	7457.217092	14.586138	-0.051317	4.654169
246.015104	7449.240913	14.591143	-0.051308	4.651755
245.749593	7441.179528	14.596147	-0.051254	4.649315
245.699672	7433.251863	14.601152	-0.051240	4.646914
245.698263	7425.138930	14.606157	-0.051235	4.644455
245.786810	7417.298148	14.611162	-0.051246	4.642078
245.656274	7409.243814	14.616167	-0.051217	4.639635
245.658211	7401.245444	14.621171	-0.051212	4.637207
245.582612	7393.243947	14.626176	-0.051193	4.634777
245.560498	7385.170745	14.631181	-0.051184	4.632324
245.753549	7377.143177	14.636186	-0.051215	4.629884
245.559675	7369.191189	14.641191	-0.051174	4.627465
245.511513	7361.134855	14.646195	-0.051160	4.625014
245.559548	7353.229472	14.651200	-0.051164	4.622606
245.363338	7345.143657	14.656205	-0.051123	4.620143
245.399820	7337.245603	14.661210	-0.051125	4.617736
245.376380	7329.214512	14.666215	-0.051115	4.615287
245.170856	7321.170328	14.671219	-0.051072	4.612832
245.272053	7313.150874	14.676224	-0.051086	4.610384
245.151866	7305.178669	14.681229	-0.051059	4.607949
245.223167	7297.183031	14.686234	-0.051067	4.605505
245.270488	7289.189596	14.691239	-0.051071	4.603061
245.061811	7281.162920	14.696243	-0.051027	4.600605
245.072422	7273.186228	14.701248	-0.051024	4.598163
244.970956	7265.127316	14.706253	-0.051000	4.595695
245.166533	7257.163964	14.711258	-0.051032	4.593255
244.803824	7249.058188	14.716263	-0.050959	4.590770
244.661311	7241.110138	14.721267	-0.050928	4.588331
244.957726	7233.116592	14.726272	-0.050978	4.585878
244.900953	7225.140263	14.731277	-0.050962	4.583428
244.654105	7217.136218	14.736282	-0.050911	4.580969
244.915769	7209.131092	14.741287	-0.050955	4.578508
244.604986	7201.107534	14.746291	-0.050892	4.576040
244.788014	7193.136556	14.751296	-0.050922	4.573587
244.581153	7185.084951	14.756301	-0.050878	4.571107
244.655364	7177.103660	14.761306	-0.050887	4.568649
244.643426	7169.132032	14.766311	-0.050880	4.566191
244.545665	7161.122546	14.771315	-0.050857	4.563721
244.605990	7153.193653	14.776320	-0.050863	4.561274
244.424803	7145.112353	14.781325	-0.050824	4.558779
244.430207	7137.186256	14.786330	-0.050820	4.556330
244.260740	7129.131964	14.791335	-0.050784	4.553840
244.280239	7121.123607	14.796339	-0.050782	4.551364
244.151235	7113.088092	14.801344	-0.050753	4.548877
243.998179	7105.068247	14.806349	-0.050720	4.546394
244.099500	7097.095782	14.811354	-0.050734	4.543924
244.035902	7089.123524	14.816359	-0.050717	4.541453
244.033042	7081.095899	14.821363	-0.050712	4.538964
244.151650	7073.154432	14.826368	-0.050729	4.536500
244.133091	7065.076348	14.831373	-0.050720	4.533992
244.042631	7057.091636	14.836378	-0.050699	4.531511
243.989112	7049.083978	14.841383	-0.050684	4.529023
243.890108	7041.100132	14.846387	-0.050660	4.526540
243.836456	7033.130425	14.851392	-0.050645	4.524060
243.674265	7025.100736	14.856397	-0.050610	4.521560
243.707960	7017.108170	14.861402	-0.050612	4.519070
243.761338	7009.135875	14.866407	-0.050617	4.516586
243.764788	7001.079264	14.871411	-0.050612	4.514073
243.943168	6993.021738	14.876416	-0.050640	4.511560
243.732628	6985.055822	14.881421	-0.050596	4.509073
243.319075	6977.090104	14.886426	-0.050514	4.506583
243.312376	6969.066532	14.891431	-0.050508	4.504076
243.610207	6961.072704	14.896435	-0.050559	4.501577
243.519006	6953.067753	14.901440	-0.050537	4.499072
243.319133	6945.070296	14.906445	-0.050495	4.496568
243.325704	6937.065479	14.911450	-0.050491	4.494061
243.397985	6929.036619	14.916455	-0.050499	4.491545
243.286424	6921.024983	14.921459	-0.050474	4.489032
243.195289	6913.053492	14.926464	-0.050452	4.486531
243.253713	6905.039237	14.931469	-0.050458	4.484015
243.405476	6897.086130	14.936474	-0.050481	4.481518
243.138658	6889.031585	14.941479	-0.050426	4.478985
243.062140	6881.082887	14.946483	-0.050407	4.476485
243.149854	6873.083305	14.951488	-0.050419	4.473969
242.938498	6865.021134	14.956493	-0.050374	4.471430
242.972380	6857.050034	14.961498	-0.050376	4.468919
242.750285	6849.046743	14.966503	-0.050329	4.466396
242.647432	6841.024900	14.971507	-0.050305	4.463866
242.880310	6833.033331	14.976512	-0.050344	4.461345
242.694103	6825.008755	14.981517	-0.050304	4.458811
242.715919	6817.026775	14.986522	-0.050303	4.456290
242.661716	6809.012736	14.991527	-0.050288	4.453757
242.739096	6800.964115	14.996531	-0.050298	4.451212
242.656273	6793.012880	15.001536	-0.050277	4.448695
242.489330	6785.001236	15.006541	-0.050241	4.446158
242.493782	6777.017581	15.011546	-0.050237	4.443629
242.617203	6769.063464	15.016551	-0.050255	4.441108
242.645714	6761.017690	15.021555	-0.050255	4.438557
242.610167	6753.032503	15.026560	-0.050244	4.436022
242.434958	6744.949667	15.031565	-0.050206	4.433455
242.366523	6736.959468	15.036570	-0.050189	4.430916
242.215285	6728.936786	15.041575	-0.050155	4.428365
242.200150	6720.920731	15.046579	-0.050148	4.425816
242.228126	6712.990068	15.051584	-0.050148	4.423292
241.990119	6704.974805	15.056589	-0.050099	4.420738
242.039362	6696.986358	15.061594	-0.050103	4.418193
242.075122	6688.980193	15.066599	-0.050105	4.415641
241.879208	6680.951929	15.071603	-0.050063	4.413079
242.020022	6672.938746	15.076608	-0.050084	4.410522
241.866102	6664.948550	15.081613	-0.050051	4.407970
241.882345	6656.972022	15.086618	-0.050049	4.405421
241.881671	6648.971102	15.091623	-0.050044	4.402863
241.910732	6640.962642	15.096627	-0.050044	4.400301
241.904189	6633.044264	15.101632	-0.050038	4.397766
241.653576	6625.007916	15.106637	-0.049987	4.395191
241.671404	6617.035090	15.111642	-0.049985	4.392636
241.746058	6608.912136	15.116647	-0.049994	4.390031
241.693313	6600.952821	15.121651	-0.049979	4.387477
241.585559	6592.969006	15.126656	-0.049954	4.384913
241.748934	6584.969511	15.131661	-0.049980	4.382345
241.710951	6576.984120	15.136666	-0.049968	4.379778
241.653867	6569.044540	15.141671	-0.049952	4.377224
241.472786	6560.940249	15.146675	-0.049913	4.374615
241.422089	6552.972199	15.151680	-0.049899	4.372049
241.293630	6544.953168	15.156685	-0.049870	4.369464
241.317509	6536.980569	15.161690	-0.049870	4.366894
241.291874	6528.985556	15.166695	-0.049860	4.364315
241.117103	6521.032033	15.171699	-0.049822	4.361747
241.254543	6513.009488	15.176704	-0.049843	4.359157
241.186066	6505.001543	15.181709	-0.049825	4.356569
241.126986	6496.958628	15.186714	-0.049809	4.353968
241.115493	6488.867494	15.191719	-0.049802	4.351350
241.196668	6480.827555	15.196723	-0.049812	4.348748
241.083423	6472.938050	15.201728	-0.049786	4.346192
240.942944	6464.932473	15.206733	-0.049755	4.343596
240.988896	6456.971136	15.211738	-0.049759	4.341015
240.996035	6448.975913	15.216743	-0.049755	4.338420
240.814263	6440.956835	15.221747	-0.049716	4.335815
240.890924	6432.993758	15.226752	-0.049726	4.333229
240.680445	6424.920696	15.231757	-0.049682	4.330603
240.721659	6416.935365	15.236762	-0.049684	4.328006
240.579332	6408.933955	15.241767	-0.049653	4.325400
240.585832	6400.941769	15.246771	-0.049649	4.322797
240.754337	6392.966072	15.251776	-0.049676	4.320200
240.698694	6384.996382	15.256781	-0.049660	4.317601
240.394355	6376.928174	15.261786	-0.049599	4.314966
240.469090	6368.894494	15.266791	-0.049608	4.312344
240.271552	6360.903558	15.271795	-0.049566	4.309732
240.218264	6352.964767	15.276800	-0.049551	4.307136
240.216457	6344.913148	15.281805	-0.049546	4.304503
240.100165	6336.943589	15.286810	-0.049519	4.301894
239.936071	6328.903824	15.291815	-0.049484	4.299260
240.045256	6320.930047	15.296819	-0.049499	4.296648
240.055650	6312.933040	15.301824	-0.049496	4.294026
239.992256	6304.879953	15.306829	-0.049479	4.291384
240.109639	6296.876801	15.311834	-0.049496	4.288758
239.990870	6288.926239	15.316839	-0.049469	4.286145
239.970642	6280.883132	15.321843	-0.049460	4.283501
239.805771	6272.960670	15.326848	-0.049425	4.280894
239.794289	6264.911136	15.331853	-0.049418	4.278245
240.146327	6256.901752	15.336858	-0.049478	4.275611
240.132503	6248.915222	15.341863	-0.049471	4.272980
240.018176	6240.855794	15.346867	-0.049445	4.270322
239.999168	6232.905826	15.351872	-0.049436	4.267699
239.926544	6224.840218	15.356877	-0.049418	4.265036
239.817645	6216.913888	15.361882	-0.049392	4.262417
239.682080	6208.896881	15.366887	-0.049362	4.259766
239.614445	6200.887798	15.371891	-0.049345	4.257116
239.663746	6192.912598	15.376896	-0.049349	4.254478
239.640766	6184.869866	15.381901	-0.049340	4.251814
239.567547	6176.876915	15.386906	-0.049321	4.249165
239.337432	6168.912203	15.391911	-0.049273	4.246522
239.164769	6160.895425	15.396915	-0.049236	4.243861
239.346805	6152.923521	15.401920	-0.049265	4.241217
239.073376	6144.946040	15.406925	-0.049209	4.238564
239.103390	6136.942411	15.411930	-0.049210	4.235904
239.215631	6128.941425	15.416935	-0.049226	4.233244
239.157086	6120.865064	15.421939	-0.049210	4.230556
239.146258	6112.920867	15.426944	-0.049203	4.227910
238.826185	6104.886819	15.431949	-0.049138	4.225230
239.048521	6096.913025	15.436954	-0.049175	4.222574
239.060881	6088.915835	15.441959	-0.049172	4.219906
238.874906	6080.944632	15.446963	-0.049133	4.217242
238.908735	6072.958809	15.451968	-0.049134	4.214575
238.787205	6064.876335	15.456973	-0.049106	4.211872
238.815453	6056.890615	15.461978	-0.049107	4.209201
238.887066	6048.940324	15.466983	-0.049115	4.206541
238.921845	6040.907657	15.471987	-0.049117	4.203851
238.745684	6032.977053	15.476992	-0.049079	4.201191
238.648938	6024.909450	15.481997	-0.049056	4.198485
238.807464	6016.947834	15.487002	-0.049081	4.195815
238.528114	6008.858315	15.492007	-0.049024	4.193096
238.324821	6000.775445	15.497011	-0.048981	4.190378
238.496402	5992.856626	15.502016	-0.049008	4.187717
238.421005	5984.871933	15.507021	-0.048989	4.185030
238.485562	5976.909163	15.512026	-0.048996	4.182350
238.380672	5968.893111	15.517031	-0.048971	4.179649
238.333991	5960.945182	15.522035	-0.048958	4.176969
238.451772	5952.903465	15.527040	-0.048975	4.174258
238.248851	5944.856373	15.532045	-0.048932	4.171539
238.286217	5936.885093	15.537050	-0.048934	4.168848
238.184137	5928.889494	15.542055	-0.048910	4.166144
237.961524	5920.884772	15.547059	-0.048864	4.163435
238.098199	5912.931186	15.552064	-0.048884	4.160745
238.075317	5904.883106	15.557069	-0.048875	4.158019
238.122006	5896.883048	15.562074	-0.048879	4.155309
238.023655	5888.892317	15.567079	-0.048855	4.152599
237.712418	5880.818624	15.572083	-0.048793	4.149856
237.762314	5872.875602	15.577088	-0.048797	4.147159
237.668664	5864.866556	15.582093	-0.048775	4.144437
237.843406	5856.912955	15.587098	-0.048802	4.141736
237.955215	5848.855717	15.592103	-0.048818	4.138996
237.792898	5840.884214	15.597107	-0.048783	4.136281
237.836624	5832.877597	15.602112	-0.048786	4.133554
237.629233	5824.827683	15.607117	-0.048742	4.130807
237.594953	5816.847354	15.612122	-0.048731	4.128085
237.528283	5808.846980	15.617127	-0.048714	4.125354
237.616690	5800.896480	15.622131	-0.048725	4.122639
237.611191	5792.867000	15.627136	-0.048719	4.119895
237.234617	5784.897775	15.632141	-0.048644	4.117165
237.348773	5776.880959	15.637146	-0.048661	4.114423
237.338852	5768.872298	15.642151	-0.048654	4.111680
237.216910	5760.817675	15.647155	-0.048626	4.108918
237.118986	5752.899580	15.652160	-0.048603	4.106202
237.134577	5744.832360	15.657165	-0.048601	4.103434
237.206287	5736.892040	15.662170	-0.048609	4.100708
237.175382	5728.905531	15.667175	-0.048599	4.097964
236.939105	5720.882441	15.672179	-0.048550	4.095202
236.988597	5712.860070	15.677184	-0.048554	4.092443
236.982670	5704.847988	15.682189	-0.048548	4.089684
236.753367	5696.898132	15.687194	-0.048500	4.086942
236.734875	5688.905536	15.692199	-0.048492	4.084186
236.738412	5680.936470	15.697203	-0.048488	4.081437
236.623870	5672.945859	15.702208	-0.048461	4.078677
236.522678	5664.928555	15.707213	-0.048438	4.075906
236.458449	5656.926997	15.712218	-0.048421	4.073139
236.406176	5648.885316	15.717223	-0.048406	4.070356
236.371582	5640.889914	15.722227	-0.048395	4.067588
236.477730	5632.900519	15.727232	-0.048409	4.064822
236.265767	5624.936815	15.732237	-0.048365	4.062058
236.272065	5616.897628	15.737242	-0.048361	4.059269
236.464101	5608.935376	15.742247	-0.048392	4.056508
236.503372	5600.906678	15.747251	-0.048394	4.053720
236.422220	5592.927149	15.752256	-0.048374	4.050945
236.404523	5584.902006	15.757261	-0.048366	4.048154
236.467363	5576.905904	15.762266	-0.048373	4.045371
236.327892	5568.964201	15.767271	-0.048342	4.042603
236.238728	5560.908560	15.772275	-0.048320	4.039794
236.105899	5552.970493	15.777280	-0.048291	4.037023
235.945006	5544.906815	15.782285	-0.048256	4.034206
235.872036	5536.775347	15.787290	-0.048237	4.031365
236.076756	5528.842048	15.792295	-0.048270	4.028595
235.799265	5520.857550	15.797299	-0.048214	4.025798
235.761235	5512.893189	15.802304	-0.048202	4.023010
235.775499	5504.875935	15.807309	-0.048199	4.020202
235.751618	5496.940763	15.812314	-0.048190	4.017420
235.778461	5488.922543	15.817319	-0.048190	4.014608
235.523586	5480.876271	15.822323	-0.048138	4.011780
235.841583	5472.876751	15.827328	-0.048192	4.008975
235.653064	5464.869098	15.832333	-0.048152	4.006157
235.475417	5456.891516	15.837338	-0.048114	4.003348
235.512975	5448.947970	15.842343	-0.048116	4.000553
235.509633	5440.938292	15.847347	-0.048110	3.997732
235.433845	5432.923426	15.852352	-0.048091	3.994905
235.478340	5424.883968	15.857357	-0.048095	3.992070
235.419374	5416.853218	15.862362	-0.048079	3.989234
235.368032	5408.919739	15.867367	-0.048064	3.986431
235.261853	5400.890243	15.872371	-0.048039	3.983591
235.168669	5392.942672	15.877376	-0.048017	3.980778
235.151855	5384.919596	15.882381	-0.048009	3.977938
234.944838	5376.935017	15.887386	-0.047966	3.975106
235.269611	5368.901119	15.892391	-0.048021	3.972263
235.172423	5360.884978	15.897395	-0.047998	3.969418
235.171226	5352.935984	15.902400	-0.047993	3.966596
235.026158	5344.916970	15.907405	-0.047961	3.963745
235.082835	5336.945004	15.912410	-0.047967	3.960911
234.908954	5328.976701	15.917415	-0.047929	3.958073
234.887494	5320.978752	15.922419	-0.047920	3.955226
235.108690	5312.911698	15.927424	-0.047957	3.952355
234.786495	5304.884856	15.932429	-0.047892	3.949488
234.726688	5296.914959	15.937434	-0.047876	3.946643
234.732192	5288.930143	15.942439	-0.047872	3.943792
234.739830	5280.957113	15.947443	-0.047868	3.940943
234.725890	5272.981322	15.952448	-0.047861	3.938091
234.449600	5264.998235	15.957453	-0.047804	3.935229
234.573556	5256.958347	15.962458	-0.047822	3.932352
234.703856	5248.947492	15.967463	-0.047842	3.929484
234.465949	5240.963615	15.972467	-0.047792	3.926616
234.499534	5232.987587	15.977472	-0.047794	3.923754
234.537570	5224.974566	15.982477	-0.047796	3.920877
234.370118	5216.973557	15.987482	-0.047760	3.917998
234.159015	5208.988550	15.992487	-0.047715	3.915122
234.024170	5200.937961	15.997491	-0.047685	3.912222
234.193069	5192.947044	16.002496	-0.047712	3.909346
234.059152	5184.968099	16.007501	-0.047682	3.906468
234.175266	5176.945770	16.012506	-0.047699	3.903576
234.184785	5168.959108	16.017511	-0.047695	3.900693
233.783987	5160.994655	16.022515	-0.047616	3.897808
233.936570	5152.987340	16.027520	-0.047639	3.894915
233.694005	5144.934307	16.032525	-0.047589	3.891997
233.667096	5136.958745	16.037530	-0.047579	3.889108
233.598117	5129.012031	16.042535	-0.047562	3.886227
233.774241	5120.962650	16.047539	-0.047589	3.883312
233.858036	5112.960304	16.052544	-0.047600	3.880409
233.497378	5105.017006	16.057549	-0.047528	3.877517
233.598921	5096.981034	16.062554	-0.047542	3.874599
233.689279	5088.727752	16.067559	-0.047554	3.871598
233.526817	5080.798054	16.072563	-0.047518	3.868709
233.672394	5072.883271	16.077568	-0.047541	3.865828
233.434223	5064.922552	16.082573	-0.047491	3.862921
233.401137	5056.937859	16.087578	-0.047480	3.860008
233.451048	5048.982853	16.092583	-0.047485	3.857104
233.439435	5040.956080	16.097587	-0.047478	3.854171
233.368344	5032.976280	16.102592	-0.047459	3.851252
233.280847	5024.923317	16.107597	-0.047438	3.848303
233.347055	5016.945532	16.112602	-0.047446	3.845383
233.303739	5009.002061	16.117607	-0.047433	3.842470
232.965549	5000.994431	16.122611	-0.047365	3.839526
233.098882	4993.022602	16.127616	-0.047385	3.836603
233.100079	4985.018403	16.132621	-0.047380	3.833663
233.136942	4977.003894	16.137626	-0.047382	3.830717
233.196562	4968.977277	16.142631	-0.047388	3.827765
233.032488	4960.976408	16.147635	-0.047352	3.824816
233.058992	4953.017430	16.152640	-0.047352	3.821884
232.921632	4945.026600	16.157645	-0.047322	3.818934
232.903904	4937.055391	16.162650	-0.047314	3.815992
233.030814	4929.062525	16.167655	-0.047332	3.813042
232.656109	4921.038270	16.172659	-0.047258	3.810068
232.826012	4913.082310	16.177664	-0.047284	3.807129
232.631952	4905.055952	16.182669	-0.047243	3.804153
232.444752	4897.113054	16.187674	-0.047203	3.801207
232.602348	4889.087905	16.192679	-0.047228	3.798234
232.500235	4881.071718	16.197683	-0.047204	3.795258
232.423882	4873.046056	16.202688	-0.047185	3.792275
232.340173	4864.996117	16.207693	-0.047164	3.789282
232.363908	4857.027549	16.212698	-0.047164	3.786318
232.301214	4849.073747	16.217703	-0.047147	3.783356
232.412052	4841.032008	16.222707	-0.047163	3.780363
232.449795	4833.080522	16.227712	-0.047165	3.777399
232.295141	4825.045701	16.232717	-0.047131	3.774398
232.076051	4817.074740	16.237722	-0.047085	3.771416
232.116361	4809.040951	16.242727	-0.047088	3.768415
232.053076	4801.054085	16.247731	-0.047071	3.765426
232.169543	4793.088428	16.252736	-0.047088	3.762447
232.141638	4785.067931	16.257741	-0.047078	3.759442
231.778839	4777.152754	16.262746	-0.047005	3.756466
232.035966	4769.081751	16.267751	-0.047048	3.753443
231.794815	4761.073814	16.272755	-0.046998	3.750431
231.737006	4753.094230	16.277760	-0.046983	3.747430
231.823725	4745.042350	16.282765	-0.046994	3.744404
231.757946	4737.109296	16.287770	-0.046977	3.741416
231.829660	4729.107709	16.292775	-0.046985	3.738403
231.603294	4721.119737	16.297779	-0.046938	3.735386
231.512294	4713.139694	16.302784	-0.046916	3.732373
231.446515	4705.094303	16.307789	-0.046899	3.729333
231.544928	4697.121854	16.312794	-0.046912	3.726322
231.449727	4689.136809	16.317799	-0.046890	3.723299
231.363765	4681.132150	16.322803	-0.046869	3.720267
231.326634	4673.195174	16.327808	-0.046857	3.717259
231.225662	4665.182338	16.332813	-0.046833	3.714218
231.251398	4657.053634	16.337818	-0.046833	3.711134
231.345918	4649.093198	16.342823	-0.046845	3.708113
231.101783	4641.099632	16.347827	-0.046795	3.705068
231.435572	4633.139093	16.352832	-0.046852	3.702048
231.197295	4625.133758	16.357837	-0.046803	3.698994
230.998304	4617.206275	16.362842	-0.046761	3.695968
230.960474	4609.184779	16.367847	-0.046749	3.692908
230.788742	4601.126454	16.372851	-0.046712	3.689828
230.810718	4593.196106	16.377856	-0.046711	3.686799
230.820593	4585.167782	16.382861	-0.046708	3.683730
230.647033	4577.227665	16.387866	-0.046671	3.680687
230.633488	4569.228931	16.392871	-0.046663	3.677623
230.613584	4561.198218	16.397875	-0.046655	3.674545
230.673867	4553.191651	16.402880	-0.046661	3.671475
230.589434	4545.168979	16.407885	-0.046640	3.668393
230.512416	4537.183454	16.412890	-0.046621	3.665322
230.696298	4529.208109	16.417895	-0.046650	3.662260
230.617208	4521.208552	16.422899	-0.046631	3.659179
230.514346	4513.278957	16.427904	-0.046607	3.656121
230.356497	4505.221389	16.432909	-0.046572	3.653010
230.386331	4497.194313	16.437914	-0.046573	3.649914
230.270842	4489.242188	16.442919	-0.046546	3.646839
230.044505	4481.230985	16.447923	-0.046499	3.643737
230.227893	4473.269426	16.452928	-0.046529	3.640662
230.186584	4465.268812	16.457933	-0.046516	3.637563
230.177830	4457.248623	16.462938	-0.046509	3.634454
230.009061	4449.204598	16.467943	-0.046473	3.631330
229.920681	4441.186890	16.472947	-0.046451	3.628215
230.200546	4433.213800	16.477952	-0.046499	3.625125
230.056611	4425.260269	16.482957	-0.046467	3.622028
230.013060	4417.241600	16.487962	-0.046454	3.618906
229.712305	4409.294484	16.492967	-0.046393	3.615802
229.686450	4401.257245	16.497971	-0.046383	3.612668
229.850119	4393.233547	16.502976	-0.046409	3.609542
229.654883	4385.266231	16.507981	-0.046367	3.606425
229.615144	4377.303587	16.512986	-0.046355	3.603311
229.648688	4369.339418	16.517991	-0.046356	3.600196
229.381737	4361.337530	16.522995	-0.046302	3.597056
229.355866	4353.357273	16.528000	-0.046292	3.593927
229.356447	4345.327181	16.533005	-0.046287	3.590778
229.525341	4337.315024	16.538010	-0.046314	3.587637
229.612318	4329.331633	16.543015	-0.046325	3.584502
229.227149	4321.370458	16.548019	-0.046248	3.581360
229.236929	4313.376572	16.553024	-0.046245	3.578214
229.253430	4305.378930	16.558029	-0.046243	3.575064
229.265790	4297.366480	16.563034	-0.046241	3.571905
229.239864	4289.364720	16.568039	-0.046231	3.568746
229.140264	4281.371538	16.573043	-0.046207	3.565585
229.180243	4273.409914	16.578048	-0.046210	3.562439
229.082894	4265.402392	16.583053	-0.046187	3.559267
229.171830	4257.435504	16.588058	-0.046198	3.556114
229.235716	4249.335033	16.593063	-0.046205	3.552905
228.981452	4241.293905	16.598067	-0.046153	3.549706
228.865985	4233.335407	16.603072	-0.046127	3.546542
228.797100	4225.361736	16.608077	-0.046109	3.543371
228.649013	4217.389429	16.613082	-0.046076	3.540194
228.632656	4209.437929	16.618087	-0.046068	3.537027
228.719876	4201.392568	16.623091	-0.046080	3.533823
228.559320	4193.404529	16.628096	-0.046045	3.530632
228.477044	4185.394401	16.633101	-0.046025	3.527431
228.394564	4177.397848	16.638106	-0.046004	3.524232
228.450313	4169.481512	16.643111	-0.046010	3.521067
228.343042	4161.471741	16.648115	-0.045985	3.517857
228.512536	4153.460558	16.653120	-0.046011	3.514651
228.446981	4145.456021	16.658125	-0.045994	3.511438
228.418669	4137.424883	16.663130	-0.045984	3.508213
228.366301	4129.432516	16.668135	-0.045969	3.505000
228.379328	4121.461835	16.673139	-0.045967	3.501794
228.378672	4113.485561	16.678144	-0.045962	3.498583
228.414630	4105.505247	16.683149	-0.045963	3.495368
228.345166	4097.517284	16.688154	-0.045946	3.492144
228.204875	4089.510587	16.693159	-0.045915	3.488907
227.981827	4081.517885	16.698163	-0.045868	3.485670
227.956416	4073.563457	16.703168	-0.045858	3.482452
227.789605	4065.573593	16.708173	-0.045822	3.479212
227.794548	4057.584606	16.713178	-0.045818	3.475975
227.924257	4049.555481	16.718183	-0.045838	3.472722
227.875320	4041.511119	16.723187	-0.045823	3.469455
227.663977	4033.572530	16.728192	-0.045779	3.466222
227.505339	4025.568197	16.733197	-0.045745	3.462961
227.672815	4017.534657	16.738202	-0.045771	3.459696
227.767276	4009.591058	16.743207	-0.045784	3.456462
227.616615	4001.560575	16.748211	-0.045751	3.453181
227.570876	3993.590485	16.753216	-0.045737	3.449925
227.592855	3985.599565	16.758221	-0.045736	3.446660
227.541083	3977.609217	16.763226	-0.045722	3.443390
227.215449	3969.667008	16.768231	-0.045656	3.440127
227.088165	3961.686656	16.773235	-0.045628	3.436852
227.316499	3953.668236	16.778240	-0.045665	3.433570
227.087812	3945.632431	16.783245	-0.045618	3.430263
227.126705	3937.606853	16.788250	-0.045620	3.426966
227.035294	3929.654298	16.793255	-0.045598	3.423691
227.127455	3921.663975	16.798259	-0.045610	3.420403
227.210851	3913.678234	16.803264	-0.045621	3.417114
227.260963	3905.665844	16.808269	-0.045625	3.413810
227.022330	3897.679844	16.813274	-0.045576	3.410503
226.935477	3889.704941	16.818279	-0.045555	3.407203
227.005540	3881.696084	16.823283	-0.045563	3.403891
227.057519	3873.734168	16.828288	-0.045567	3.400595
226.983465	3865.755128	16.833293	-0.045549	3.397284
226.846941	3857.742529	16.838298	-0.045518	3.393954
226.795051	3849.658642	16.843303	-0.045504	3.390594
226.599002	3841.691741	16.848307	-0.045462	3.387274
226.527487	3833.728226	16.853312	-0.045444	3.383956
226.579717	3825.747104	16.858317	-0.045449	3.380633
226.540701	3817.787538	16.863322	-0.045437	3.377312
226.154947	3809.806264	16.868327	-0.045360	3.373966
226.205987	3801.745838	16.873331	-0.045364	3.370599
226.567740	3793.760142	16.878336	-0.045427	3.367271
226.407419	3785.787378	16.883341	-0.045392	3.363927
226.476451	3777.811130	16.888346	-0.045400	3.360586
226.505232	3769.875251	16.893351	-0.045400	3.357257
226.355942	3761.842223	16.898355	-0.045368	3.353878
226.455120	3753.808518	16.903360	-0.045381	3.350504
226.334669	3745.829312	16.908365	-0.045354	3.347142
226.134816	3737.848780	16.913370	-0.045312	3.343773
226.066911	3729.894512	16.918375	-0.045294	3.340416
226.053172	3721.883678	16.923379	-0.045287	3.337034
226.253559	3713.871132	16.928384	-0.045319	3.333655
225.888724	3705.856348	16.933389	-0.045246	3.330252
225.814217	3697.894470	16.938394	-0.045227	3.326878
225.842117	3689.918452	16.943399	-0.045228	3.323498
225.677180	3681.939584	16.948403	-0.045192	3.320107
225.537868	3673.997545	16.953408	-0.045161	3.316729
225.773574	3665.931390	16.958413	-0.045200	3.313308
225.733849	3657.889824	16.963418	-0.045188	3.309884
225.615085	3649.952984	16.968423	-0.045161	3.306498
225.463234	3641.955577	16.973427	-0.045127	3.303082
225.571111	3633.988646	16.978432	-0.045142	3.299685
225.430398	3626.035323	16.983437	-0.045111	3.296281
225.467832	3618.007206	16.988442	-0.045113	3.292848
225.502378	3610.003736	16.993447	-0.045115	3.289422
225.341692	3602.030541	16.998451	-0.045080	3.285997
225.360364	3594.056094	17.003456	-0.045079	3.282576
225.050516	3586.079720	17.008461	-0.045016	3.279137
224.983268	3578.094955	17.013466	-0.044998	3.275701
225.275180	3570.055537	17.018471	-0.045048	3.272252
225.206442	3562.039911	17.023475	-0.045030	3.268795
225.303846	3554.048746	17.028480	-0.045043	3.265351
225.132707	3546.090517	17.033485	-0.045006	3.261907
224.940111	3538.117480	17.038490	-0.044966	3.258453
224.867948	3530.144824	17.043495	-0.044947	3.255000
224.722241	3522.121171	17.048499	-0.044915	3.251518
224.669564	3514.119913	17.053504	-0.044900	3.248045
224.744882	3506.113978	17.058509	-0.044910	3.244572
224.870838	3498.154251	17.063514	-0.044928	3.241118
224.875018	3490.188432	17.068519	-0.044924	3.237652
224.661248	3482.179766	17.073523	-0.044879	3.234155
224.806796	3474.116343	17.078528	-0.044901	3.230645
224.658564	3466.162665	17.083533	-0.044869	3.227167
224.276592	3458.208795	17.088538	-0.044793	3.223676
224.378740	3450.224773	17.093543	-0.044807	3.220187
224.277384	3442.224296	17.098547	-0.044783	3.216680
224.372743	3434.211237	17.103552	-0.044796	3.213170
224.171015	3426.234907	17.108557	-0.044753	3.209661
224.275708	3418.249806	17.113562	-0.044768	3.206157
224.136367	3410.285854	17.118567	-0.044737	3.202648
224.004629	3402.298094	17.123571	-0.044708	3.199125
224.078856	3394.342083	17.128576	-0.044716	3.195621
223.992199	3386.311111	17.133581	-0.044695	3.192074
224.010437	3378.281216	17.138586	-0.044694	3.188527
223.963617	3370.320794	17.143591	-0.044680	3.185004
224.051085	3362.331669	17.148595	-0.044691	3.181470
223.894515	3354.372708	17.153600	-0.044657	3.177935
223.728936	3346.382769	17.158605	-0.044622	3.174382
223.767306	3338.379382	17.163610	-0.044624	3.170828
223.803264	3330.391498	17.168615	-0.044626	3.167277
223.617468	3322.406701	17.173619	-0.044586	3.163714
223.579688	3314.438332	17.178624	-0.044574	3.160160
223.682290	3306.466700	17.183629	-0.044588	3.156607
223.664610	3298.436797	17.188634	-0.044580	3.153018
223.509143	3290.446932	17.193639	-0.044546	3.149438
223.275035	3282.470439	17.198643	-0.044498	3.145855
223.477335	3274.479878	17.203648	-0.044530	3.142282
223.272915	3266.524334	17.208653	-0.044487	3.138702
223.120965	3258.540172	17.213658	-0.044454	3.135108
223.206024	3250.543273	17.218663	-0.044465	3.131514
223.124426	3242.504078	17.223667	-0.044445	3.127890
223.206021	3234.531447	17.228672	-0.044455	3.124299
223.153036	3226.595801	17.233677	-0.044440	3.120714
222.939750	3218.613424	17.238682	-0.044396	3.117097
223.036844	3210.598497	17.243687	-0.044409	3.113475
223.049982	3202.573673	17.248691	-0.044406	3.109840
223.064230	3194.613152	17.253696	-0.044404	3.106230
222.844458	3186.627583	17.258701	-0.044358	3.102594
222.858847	3178.656829	17.263706	-0.044356	3.098972
222.813148	3170.682919	17.268711	-0.044342	3.095340
222.847396	3162.652138	17.273715	-0.044344	3.091683
222.784358	3154.691954	17.278720	-0.044327	3.088048
222.775250	3146.690637	17.283725	-0.044321	3.084393
222.762538	3138.730563	17.288730	-0.044313	3.080753
222.798033	3130.762748	17.293735	-0.044315	3.077107
222.637364	3122.732406	17.298739	-0.044280	3.073418
222.594021	3114.669245	17.303744	-0.044267	3.069716
222.450967	3106.725830	17.308749	-0.044235	3.066059
222.458245	3098.743363	17.313754	-0.044232	3.062388
222.584594	3090.790789	17.318759	-0.044250	3.058731
222.191784	3082.842069	17.323763	-0.044172	3.055047
222.184484	3074.825662	17.328768	-0.044166	3.051345
222.222329	3066.822436	17.333773	-0.044168	3.047648
222.334466	3058.828655	17.338778	-0.044184	3.043954
222.007939	3050.909400	17.343783	-0.044118	3.040268
221.825395	3042.923804	17.348787	-0.044080	3.036555
222.125774	3034.890569	17.353792	-0.044130	3.032838
221.900858	3026.907554	17.358797	-0.044084	3.029114
221.860697	3018.923268	17.363802	-0.044071	3.025394
221.965083	3010.965862	17.368807	-0.044086	3.021689
221.964643	3002.972978	17.373811	-0.044081	3.017958
221.761809	2995.005837	17.378816	-0.044038	3.014225
221.658885	2986.996853	17.383821	-0.044014	3.010472
221.846094	2978.984058	17.388826	-0.044044	3.006726
221.851724	2971.030867	17.393831	-0.044040	3.002996
221.598246	2963.064414	17.398835	-0.043988	2.999241
221.779638	2955.082004	17.403840	-0.044017	2.995496
221.694076	2947.067520	17.408845	-0.043996	2.991718
221.346697	2939.095615	17.413850	-0.043926	2.987942
221.332119	2931.099920	17.418855	-0.043919	2.984166
221.275320	2923.138648	17.423859	-0.043903	2.980400
221.399835	2915.171426	17.428864	-0.043921	2.976636
221.158426	2907.184850	17.433869	-0.043871	2.972839
221.111751	2899.183155	17.438874	-0.043858	2.969040
220.982303	2891.207170	17.443879	-0.043829	2.965243
221.127579	2883.213919	17.448883	-0.043851	2.961448
221.233844	2875.258618	17.453888	-0.043866	2.957664
220.992104	2867.277045	17.458893	-0.043816	2.953845
220.835797	2859.250310	17.463898	-0.043782	2.950004
220.959070	2851.286068	17.468903	-0.043800	2.946202
220.821172	2843.284116	17.473907	-0.043769	2.942364
220.762831	2835.336750	17.478912	-0.043753	2.938550
220.639803	2827.375572	17.483917	-0.043725	2.934722
220.659257	2819.342467	17.488922	-0.043724	2.930862
220.712651	2811.365493	17.493927	-0.043729	2.927025
220.530531	2803.400756	17.498931	-0.043690	2.923177
220.654129	2795.440907	17.503936	-0.043708	2.919342
220.464204	2787.483250	17.508941	-0.043668	2.915487
220.399654	2779.401217	17.513946	-0.043651	2.911573
220.424684	2771.414230	17.518951	-0.043651	2.907704
220.072702	2763.447304	17.523955	-0.043580	2.903820
220.147288	2755.493526	17.528960	-0.043589	2.899960
220.184295	2747.512771	17.533965	-0.043591	2.896080
219.939555	2739.534874	17.538970	-0.043541	2.892180
219.922817	2731.550209	17.543975	-0.043533	2.888285
219.913139	2723.554462	17.548979	-0.043526	2.884379
220.205668	2715.600920	17.553984	-0.043576	2.880505
220.096806	2707.641596	17.558989	-0.043550	2.876601
219.934953	2699.642447	17.563994	-0.043515	2.872669
219.809973	2691.677520	17.568999	-0.043487	2.868750
219.721106	2683.656683	17.574003	-0.043466	2.864801
219.544379	2675.723354	17.579008	-0.043428	2.860885
219.490509	2667.748552	17.584013	-0.043413	2.856949
219.577769	2659.736621	17.589018	-0.043424	2.852997
219.576408	2651.759639	17.594023	-0.043419	2.849053
219.324645	2643.789926	17.599027	-0.043367	2.845092
219.479399	2635.828121	17.604032	-0.043391	2.841153
219.438900	2627.865530	17.609037	-0.043379	2.837197
219.263736	2619.867280	17.614042	-0.043341	2.833210
219.227375	2611.867693	17.619047	-0.043329	2.829224
219.228182	2603.870147	17.624051	-0.043324	2.825236
219.421214	2595.893142	17.629056	-0.043355	2.821264
219.325445	2587.935401	17.634061	-0.043333	2.817279
219.300629	2579.945940	17.639066	-0.043323	2.813276
219.135670	2571.980862	17.644071	-0.043288	2.809272
219.039966	2563.997513	17.649075	-0.043265	2.805257
219.205408	2556.020953	17.654080	-0.043291	2.801255
218.933668	2548.077719	17.659085	-0.043235	2.797239
218.765273	2540.091404	17.664090	-0.043199	2.793201
218.886150	2532.093077	17.669095	-0.043216	2.789168
218.766795	2524.100226	17.674099	-0.043189	2.785118
218.641867	2516.165285	17.679104	-0.043161	2.781091
218.678170	2508.191144	17.684109	-0.043163	2.777047
218.770045	2500.170531	17.689114	-0.043175	2.772978
218.570134	2492.221497	17.694119	-0.043133	2.768921
218.588879	2484.218826	17.699123	-0.043131	2.764845
218.500644	2476.286951	17.704128	-0.043110	2.760792
218.297938	2468.358243	17.709133	-0.043067	2.756727
218.326504	2460.289177	17.714138	-0.043068	2.752599
218.217418	2452.296499	17.719143	-0.043043	2.748496
218.179346	2444.314118	17.724147	-0.043031	2.744395
218.056398	2436.374958	17.729152	-0.043003	2.740306
217.958753	2428.407155	17.734157	-0.042980	2.736198
218.017219	2420.403211	17.739162	-0.042986	2.732074
218.059807	2412.429511	17.744167	-0.042989	2.727958
218.054230	2404.437361	17.749171	-0.042983	2.723824
217.907720	2396.500643	17.754176	-0.042950	2.719704
217.832795	2388.553656	17.759181	-0.042932	2.715576
217.691089	2380.561938	17.764186	-0.042900	2.711415
217.607894	2372.589944	17.769191	-0.042880	2.707261
217.678941	2364.584191	17.774195	-0.042888	2.703093
217.673909	2356.638133	17.779200	-0.042882	2.698945
217.476972	2348.692781	17.784205	-0.042841	2.694778
217.414763	2340.675668	17.789210	-0.042824	2.690577
217.521512	2332.694132	17.794215	-0.042839	2.686397
217.322727	2324.752995	17.799219	-0.042797	2.682214
217.433363	2316.783913	17.804224	-0.042813	2.678028
217.358485	2308.808287	17.809229	-0.042794	2.673821
217.184710	2300.802299	17.814234	-0.042757	2.669585
217.249562	2292.822564	17.819239	-0.042764	2.665371
217.156881	2284.851042	17.824243	-0.042742	2.661145
217.255169	2276.899507	17.829248	-0.042755	2.656935
216.912129	2268.937541	17.834253	-0.042686	2.652684
216.785883	2260.952598	17.839258	-0.042658	2.648428
216.833809	2252.988466	17.844263	-0.042662	2.644188
216.722463	2245.027713	17.849267	-0.042636	2.639932
216.701112	2237.073743	17.854272	-0.042627	2.635679
216.792908	2229.045555	17.859277	-0.042639	2.631386
216.563777	2221.084276	17.864282	-0.042592	2.627102
216.651946	2213.134341	17.869287	-0.042603	2.622837
216.423796	2205.177023	17.874291	-0.042556	2.618541
216.627985	2197.185931	17.879296	-0.042589	2.614248
216.375329	2189.216624	17.884301	-0.042537	2.609929
216.330993	2181.242525	17.889306	-0.042524	2.605614
216.528171	2173.278344	17.894311	-0.042555	2.601314
216.418614	2165.323226	17.899315	-0.042530	2.596991
216.202233	2157.281970	17.904320	-0.042485	2.592607
216.397899	2149.180797	17.909325	-0.042516	2.588211
216.328717	2141.239458	17.914330	-0.042499	2.583876
216.161561	2133.348341	17.919335	-0.042463	2.579555
215.956911	2125.406267	17.924339	-0.042420	2.575195
215.910635	2117.447565	17.929344	-0.042406	2.570831
215.841253	2109.495939	17.934349	-0.042388	2.566461
215.985152	2101.491808	17.939354	-0.042410	2.562069
215.975085	2093.577416	17.944359	-0.042403	2.557709
215.653094	2085.612030	17.949363	-0.042338	2.553292
215.739707	2077.620329	17.954368	-0.042350	2.548880
215.659371	2069.647288	17.959373	-0.042330	2.544460
215.555040	2061.703290	17.964378	-0.042305	2.540046
215.853627	2053.733017	17.969383	-0.042356	2.535639
215.800796	2045.745908	17.974387	-0.042341	2.531190
215.659622	2037.797032	17.979392	-0.042310	2.526748
215.466959	2029.872997	17.984397	-0.042269	2.522308
215.471292	2021.900966	17.989402	-0.042265	2.517847
215.503942	2013.922721	17.994407	-0.042266	2.513378
215.216917	2005.945054	17.999411	-0.042208	2.508877
215.372707	1997.949216	18.004416	-0.042232	2.504390
215.346650	1989.992452	18.009421	-0.042222	2.499904
215.251973	1982.052217	18.014426	-0.042200	2.495415
215.381272	1974.072797	18.019431	-0.042219	2.490911
214.928623	1966.147088	18.024435	-0.042130	2.486387
214.877260	1958.197179	18.029440	-0.042115	2.481870
214.911918	1950.228920	18.034445	-0.042117	2.477341
214.732000	1942.248939	18.039450	-0.042078	2.472782
214.973949	1934.240255	18.044455	-0.042118	2.468228
214.786188	1926.278299	18.049459	-0.042078	2.463661
214.694133	1918.352455	18.054464	-0.042056	2.459114
214.739834	1910.395297	18.059469	-0.042060	2.454550
214.800268	1902.390491	18.064474	-0.042066	2.449951
214.433170	1894.498235	18.069479	-0.041993	2.445377
214.582696	1886.503305	18.074483	-0.042016	2.440773
214.611930	1878.557807	18.079488	-0.042016	2.436181
214.606233	1870.524748	18.084493	-0.042010	2.431526
214.345585	1862.563582	18.089498	-0.041957	2.426884
214.306651	1854.625471	18.094503	-0.041945	2.422264
214.161963	1846.684954	18.099507	-0.041913	2.417626
214.075985	1838.721786	18.104512	-0.041892	2.412970
214.087173	1830.760057	18.109517	-0.041889	2.408313
214.152625	1822.781213	18.114522	-0.041896	2.403642
214.204587	1814.853881	18.119527	-0.041901	2.398991
213.868877	1806.916229	18.124531	-0.041834	2.394294
213.918698	1798.927228	18.129536	-0.041838	2.389588
213.799301	1790.968916	18.134541	-0.041811	2.384877
213.880042	1783.008001	18.139546	-0.041821	2.380171
213.790154	1775.084354	18.144551	-0.041799	2.375465
213.680130	1767.097817	18.149555	-0.041774	2.370710
213.631343	1759.145308	18.154560	-0.041760	2.365971
213.433629	1751.227524	18.159565	-0.041718	2.361231
213.470341	1743.271158	18.164570	-0.041720	2.356477
213.402968	1735.292040	18.169575	-0.041703	2.351692
213.163767	1727.310894	18.174579	-0.041653	2.346881
213.396121	1719.334178	18.179584	-0.041692	2.342102
213.188812	1711.425506	18.184589	-0.041648	2.337318
213.053981	1703.453332	18.189594	-0.041618	2.332492
213.302211	1695.469028	18.194599	-0.041659	2.327680
213.472542	1687.495480	18.199603	-0.041686	2.322859
213.172753	1679.601778	18.204608	-0.041625	2.318036
212.975555	1671.663809	18.209613	-0.041584	2.313186
212.937927	1663.681672	18.214618	-0.041572	2.308311
213.023553	1655.732399	18.219623	-0.041583	2.303456
212.790376	1647.804405	18.224627	-0.041535	2.298578
212.755545	1639.854183	18.229632	-0.041523	2.293692
212.705256	1631.889093	18.234637	-0.041509	2.288785
212.399321	1623.955119	18.239642	-0.041447	2.283865
212.557661	1616.009395	18.244647	-0.041472	2.278967
212.518897	1608.030110	18.249651	-0.041460	2.274020
212.252179	1600.036472	18.254656	-0.041405	2.269034
212.436546	1592.057421	18.259661	-0.041434	2.264085
212.325185	1584.123482	18.264666	-0.041409	2.259128
212.223349	1576.207940	18.269671	-0.041385	2.254173
211.880424	1568.265505	18.274675	-0.041316	2.249168
212.170946	1560.279237	18.279680	-0.041365	2.244180
212.080585	1552.370869	18.284685	-0.041343	2.239197
211.740588	1544.452984	18.289690	-0.041275	2.234174
211.911236	1536.463630	18.294695	-0.041302	2.229140
211.934525	1528.487736	18.299699	-0.041302	2.224091
211.875136	1520.577634	18.304704	-0.041286	2.219064
211.707322	1512.649997	18.309709	-0.041249	2.214004
211.759550	1504.669271	18.314714	-0.041254	2.208920
211.980835	1496.718896	18.319719	-0.041291	2.203858
211.766891	1488.804725	18.324723	-0.041246	2.198768
211.867050	1480.857338	18.329728	-0.041260	2.193673
211.828707	1472.885188	18.334733	-0.041247	2.188538
211.502295	1464.963158	18.339738	-0.041182	2.183397
211.333494	1457.062951	18.344743	-0.041145	2.178273
211.304143	1449.088986	18.349747	-0.041135	2.173101
211.164831	1441.154213	18.354752	-0.041104	2.167932
211.440896	1433.174234	18.359757	-0.041151	2.162760
211.433437	1425.247846	18.364762	-0.041144	2.157584
211.412850	1417.322331	18.369767	-0.041136	2.152395
211.127716	1409.388417	18.374771	-0.041078	2.147164
210.969374	1401.464164	18.379776	-0.041043	2.141937
211.033185	1393.527246	18.384781	-0.041050	2.136711
210.823388	1385.588590	18.389786	-0.041006	2.131444
210.943889	1377.637715	18.394791	-0.041024	2.126188
210.718694	1369.719560	18.399795	-0.040977	2.120907
210.755766	1361.787430	18.404800	-0.040979	2.115629
210.619868	1353.790719	18.409805	-0.040949	2.110278
210.561002	1345.843534	18.414810	-0.040933	2.104954
210.614751	1337.914812	18.419815	-0.040938	2.099640
210.375127	1330.009927	18.424819	-0.040888	2.094300
210.307644	1322.069624	18.429824	-0.040871	2.088939
210.387269	1314.120739	18.434829	-0.040881	2.083573
210.160041	1306.221963	18.439834	-0.040834	2.078197
210.231877	1298.282984	18.444839	-0.040842	2.072809
210.268168	1290.327199	18.449843	-0.040844	2.067392
210.192349	1282.410879	18.454848	-0.040825	2.061977
209.999586	1274.511562	18.459853	-0.040784	2.056547
209.965434	1266.550974	18.464858	-0.040773	2.051076
209.933035	1258.639440	18.469863	-0.040762	2.045625
209.729691	1250.724433	18.474867	-0.040719	2.040140
209.500928	1242.841340	18.479872	-0.040672	2.034659
209.601014	1234.854856	18.484877	-0.040686	2.029126
209.433192	1226.918365	18.489882	-0.040649	2.023584
209.253700	1219.033807	18.494887	-0.040611	2.018062
209.486582	1211.040706	18.499891	-0.040649	2.012492
209.321174	1203.125601	18.504896	-0.040614	2.006920
209.158899	1195.228574	18.509901	-0.040579	2.001345
209.133554	1187.303954	18.514906	-0.040569	1.995749
209.237424	1179.366489	18.519911	-0.040584	1.990143
209.103063	1171.446981	18.524915	-0.040554	1.984507
208.997099	1163.543187	18.529920	-0.040529	1.978871
209.092159	1155.611671	18.534925	-0.040542	1.973219
209.038989	1147.672874	18.539930	-0.040527	1.967530
209.022192	1139.772236	18.544935	-0.040519	1.961856
208.793484	1131.888290	18.549939	-0.040472	1.956155
208.808831	1123.924623	18.554944	-0.040469	1.950406
208.611384	1116.012686	18.559949	-0.040428	1.944654
208.419616	1108.110131	18.564954	-0.040387	1.938893
208.580550	1100.175532	18.569959	-0.040412	1.933129
208.310706	1092.259186	18.574963	-0.040357	1.927315
208.419603	1084.330392	18.579968	-0.040373	1.921515
208.379319	1076.440957	18.584973	-0.040360	1.915710
208.069097	1068.537865	18.589978	-0.040297	1.909848
208.088795	1060.629515	18.594983	-0.040296	1.904000
208.036799	1052.710702	18.599987	-0.040282	1.898118
207.969406	1044.804751	18.604992	-0.040264	1.892226
208.036371	1036.868991	18.609997	-0.040272	1.886309
207.766868	1028.993869	18.615002	-0.040217	1.880380
207.969856	1021.076106	18.620007	-0.040250	1.874454
207.968819	1013.126434	18.625011	-0.040245	1.868462
207.800042	1005.245792	18.630016	-0.040208	1.862484
207.574346	997.373386	18.635021	-0.040161	1.856486
207.659628	989.432453	18.640026	-0.040172	1.850452
207.606384	981.544677	18.645031	-0.040158	1.844423
207.397600	973.671801	18.650035	-0.040114	1.838367
207.390419	965.767242	18.655040	-0.040108	1.832291
207.086388	957.891532	18.660045	-0.040046	1.826182
207.210696	949.953413	18.665050	-0.040064	1.820055
207.176034	942.078452	18.670055	-0.040053	1.813937
207.097975	934.165937	18.675059	-0.040034	1.807764
206.911090	926.297914	18.680064	-0.039994	1.801591
207.082559	918.388350	18.685069	-0.040021	1.795408
206.922242	910.444445	18.690074	-0.039986	1.789136
206.838426	902.560020	18.695079	-0.039966	1.782898
206.847294	894.665999	18.700083	-0.039963	1.776643
206.993642	886.744431	18.705088	-0.039985	1.770360
206.873012	878.883825	18.710093	-0.039958	1.764070
206.432958	871.064798	18.715098	-0.039871	1.757752
206.711128	863.134501	18.720103	-0.039918	1.751411
206.539178	855.250702	18.725107	-0.039881	1.745027
206.364737	847.397600	18.730112	-0.039843	1.738645
206.463093	839.497503	18.735117	-0.039857	1.732236
206.035823	831.652506	18.740122	-0.039773	1.725781
206.175491	823.772062	18.745127	-0.039794	1.719345
205.965197	815.903996	18.750131	-0.039750	1.712850
206.075090	807.978647	18.755136	-0.039765	1.706325
205.946395	800.128242	18.760141	-0.039736	1.699805
205.800293	792.265995	18.765146	-0.039704	1.693248
205.760606	784.378452	18.770151	-0.039692	1.686659
205.816394	776.488375	18.775155	-0.039698	1.680054
205.591379	768.672247	18.780160	-0.039651	1.673448
205.631956	760.771769	18.785165	-0.039654	1.666780
205.628120	752.899390	18.790170	-0.039648	1.660103
205.581188	745.053405	18.795175	-0.039634	1.653416
205.331478	737.200571	18.800179	-0.039583	1.646668
205.342086	729.336966	18.805184	-0.039580	1.639919
205.402571	721.459743	18.810189	-0.039587	1.633137
205.210291	713.568786	18.815194	-0.039546	1.626279
205.097056	705.736041	18.820199	-0.039520	1.619455
205.116828	697.874010	18.825203	-0.039519	1.612594
204.983755	690.020652	18.830208	-0.039489	1.605690
204.936646	682.191576	18.835213	-0.039475	1.598790
204.743697	674.356675	18.840218	-0.039435	1.591834
204.633273	666.518139	18.845223	-0.039409	1.584856
204.515748	658.683714	18.850227	-0.039383	1.577850
204.618502	650.810870	18.855232	-0.039397	1.570810
204.611056	642.970864	18.860237	-0.039391	1.563752
204.441633	635.158454	18.865242	-0.039354	1.556663
204.344754	627.312211	18.870247	-0.039331	1.549521
204.282959	619.472243	18.875251	-0.039315	1.542357
203.993638	611.679121	18.880256	-0.039256	1.535169
203.881221	603.848683	18.885261	-0.039231	1.527939
203.836029	596.006887	18.890266	-0.039217	1.520674
203.919829	588.190052	18.895271	-0.039228	1.513418
203.800645	580.354307	18.900275	-0.039201	1.506077
203.691187	572.554059	18.905280	-0.039176	1.498736
203.639242	564.725571	18.910285	-0.039161	1.491340
203.447144	556.932054	18.915290	-0.039121	1.483919
203.626120	549.104600	18.920295	-0.039149	1.476486
203.450424	541.254477	18.925299	-0.039112	1.468939
203.318192	533.456429	18.930304	-0.039082	1.461409
203.203118	525.674090	18.935309	-0.039056	1.453858
203.080873	517.859628	18.940314	-0.039028	1.446235
203.217905	510.058483	18.945319	-0.039049	1.438627
203.105195	502.270498	18.950323	-0.039023	1.430950
203.083299	494.475790	18.955328	-0.039014	1.423241
202.926445	486.721427	18.960333	-0.038980	1.415507
202.764141	478.933486	18.965338	-0.038945	1.407696
202.718966	471.169443	18.970343	-0.038932	1.399885
202.668837	463.375717	18.975347	-0.038918	1.392000
202.495172	455.604196	18.980352	-0.038881	1.384071
202.407299	447.845682	18.985357	-0.038860	1.376124
202.134800	440.089292	18.990362	-0.038804	1.368102
202.149946	432.321506	18.995367	-0.038802	1.360070
201.948391	424.583849	19.000371	-0.038760	1.351985
201.859753	416.823499	19.005376	-0.038739	1.343846
202.009224	409.042535	19.010381	-0.038762	1.335678
201.835919	401.298962	19.015386	-0.038725	1.327442
201.622416	393.595533	19.020391	-0.038680	1.319191
201.638300	385.759040	19.025395	-0.038678	1.310785
201.620684	377.972919	19.030400	-0.038670	1.302374
201.362261	370.296563	19.035405	-0.038617	1.293983
201.264638	362.558229	19.040410	-0.038594	1.285500
201.305638	354.851255	19.045415	-0.038597	1.277020
201.086490	347.158859	19.050419	-0.038552	1.268452
201.006721	339.454348	19.055424	-0.038532	1.259837
200.838218	331.775740	19.060429	-0.038496	1.251176
200.739656	324.070080	19.065434	-0.038473	1.242437
200.674546	316.395043	19.070439	-0.038456	1.233677
200.518054	308.694393	19.075443	-0.038422	1.224807
200.495198	301.009313	19.080448	-0.038413	1.215917
200.368458	293.341309	19.085453	-0.038385	1.206961
200.188929	285.695460	19.090458	-0.038347	1.197953
200.281977	278.005896	19.095463	-0.038359	1.188880
200.026489	270.381764	19.100467	-0.038307	1.179745
199.813741	262.758236	19.105472	-0.038263	1.170548
199.694182	255.126975	19.110477	-0.038236	1.161287
199.576943	247.484203	19.115482	-0.038209	1.151939
199.231468	239.873573	19.120487	-0.038140	1.142505
199.182848	232.240262	19.125491	-0.038126	1.133028
198.997980	224.638092	19.130496	-0.038087	1.123481
198.865673	217.052439	19.135501	-0.038058	1.113884
198.779586	209.442378	19.140506	-0.038037	1.104182
198.705618	201.865611	19.145511	-0.038019	1.094440
198.551780	194.286097	19.150515	-0.037985	1.084589
198.181078	186.776235	19.155520	-0.037912	1.074690
198.131917	179.196595	19.160525	-0.037898	1.064680
197.892940	171.664068	19.165530	-0.037849	1.054594
197.619376	164.152003	19.170535	-0.037793	1.044430
197.406741	156.645948	19.175539	-0.037749	1.034189
197.404909	149.106823	19.180544	-0.037744	1.023850
197.282775	141.612395	19.185549	-0.037717	1.013438
196.846417	134.167042	19.190554	-0.037631	1.002911
196.785148	126.674617	19.195559	-0.037615	0.992297
196.393024	119.222192	19.200563	-0.037537	0.981544
196.221282	111.776804	19.205568	-0.037501	0.970737
196.160253	104.328074	19.210573	-0.037485	0.959832
195.961950	96.911545	19.215578	-0.037443	0.948813
195.927320	89.499115	19.220583	-0.037432	0.937715
195.389211	82.172346	19.225587	-0.037328	0.926479
195.148122	74.824437	19.230592	-0.037278	0.915153
195.304188	67.404648	19.235597	-0.037303	0.903682
194.824197	60.355915	19.240602	-0.037209	0.892473