Thu Mar 11 18:56:35 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.908307	0.063332	0.000000	0.000031	0.725270

0.940126	0.061513	0.005005	0.000025	0.725279
0.839081	0.046423	0.010010	0.000044	0.725214
0.856697	0.040187	0.015014	0.000040	0.725209
0.883245	0.039824	0.020019	0.000035	0.725218
0.785507	0.054043	0.025024	0.000053	0.725212
0.882450	0.035041	0.030029	0.000034	0.725209
0.965916	0.022989	0.035034	0.000019	0.725215
0.956760	0.019563	0.040038	0.000020	0.725206
0.963646	0.023179	0.045043	0.000018	0.725216
0.892141	0.032888	0.050048	0.000031	0.725211
1.057983	0.003417	0.055053	0.000000	0.725211
1.108429	-0.004034	0.060058	-0.000009	0.725215
0.987963	0.015029	0.065062	0.000013	0.725211
1.030066	0.010181	0.070067	0.000005	0.725216
0.997786	0.012747	0.075072	0.000010	0.725211
0.906956	0.006578	0.080077	0.000027	0.725167
1.017952	-0.154749	0.085082	0.000006	0.724891
0.762686	-0.114319	0.090086	0.000053	0.724882
0.755576	-0.108094	0.095091	0.000054	0.724892
0.614409	-0.084905	0.100096	0.000080	0.724889
0.668651	-0.094389	0.105101	0.000070	0.724890
0.868930	-0.128316	0.110106	0.000033	0.724893
0.771286	-0.156958	0.115110	0.000050	0.724804
0.548417	-0.222886	0.120115	0.000092	0.724598
0.779290	-0.266488	0.125120	0.000048	0.724593
0.798419	-0.271038	0.130125	0.000045	0.724592
0.465182	-0.208429	0.135130	0.000106	0.724599
0.512912	-0.222138	0.140134	0.000097	0.724589
0.736267	-0.406306	0.145139	0.000055	0.724307
0.846403	-0.449341	0.150144	0.000035	0.724261
0.759839	-0.435352	0.155149	0.000051	0.724259
0.671881	-0.415973	0.160154	0.000067	0.724267
0.586465	-0.496968	0.165158	0.000082	0.724079
0.737677	-0.584168	0.170163	0.000054	0.723962
0.719134	-0.585077	0.175168	0.000057	0.723954
0.633248	-0.570372	0.180173	0.000073	0.723953
0.579083	-0.677323	0.185178	0.000083	0.723725
0.676192	-0.742794	0.190182	0.000064	0.723631
0.572502	-0.721772	0.195187	0.000083	0.723637
0.380484	-0.722977	0.200192	0.000119	0.723568
0.443371	-0.851144	0.205197	0.000107	0.723339
0.585878	-0.873400	0.210202	0.000080	0.723346
0.398785	-0.845451	0.215206	0.000115	0.723336
0.335586	-0.995105	0.220211	0.000126	0.723021
0.654658	-1.060817	0.225216	0.000067	0.723004
0.582328	-1.048246	0.230221	0.000080	0.723004
0.476621	-1.180632	0.235226	0.000099	0.722708
0.301851	-1.159406	0.240230	0.000132	0.722689
0.496311	-1.213150	0.245235	0.000095	0.722652
0.371758	-1.335348	0.250240	0.000118	0.722369
0.315028	-1.326269	0.255245	0.000128	0.722368
0.657498	-1.453625	0.260250	0.000064	0.722238
0.452409	-1.502191	0.265254	0.000102	0.722071
0.341456	-1.479204	0.270259	0.000123	0.722078
0.132868	-1.602292	0.275264	0.000161	0.721764
0.216378	-1.627916	0.280269	0.000146	0.721743
0.269410	-1.705029	0.285274	0.000135	0.721611
0.187673	-1.781916	0.290278	0.000150	0.721432
0.120712	-1.778319	0.295283	0.000163	0.721416
-0.222122	-1.865922	0.300288	0.000226	0.721124
-0.278266	-1.856628	0.305293	0.000236	0.721123
-0.071486	-1.972092	0.310298	0.000198	0.720969
-0.312904	-1.978250	0.315302	0.000242	0.720873
-0.325341	-2.033151	0.320307	0.000244	0.720761
-0.554779	-2.104010	0.325312	0.000287	0.720542
-1.295332	-1.973034	0.330317	0.000424	0.720540
-1.820165	-2.027125	0.335322	0.000522	0.720251
-2.051453	-2.002415	0.340326	0.000565	0.720219
-2.185942	-1.998470	0.345331	0.000589	0.720180
-3.246836	-1.952420	0.350336	0.000787	0.719899
-3.365404	-1.931849	0.355341	0.000808	0.719898
-3.289050	-1.941593	0.360346	0.000794	0.719906
-4.041904	-1.936718	0.365350	0.000934	0.719652
-4.664527	-1.850099	0.370355	0.001049	0.719605
-4.459436	-1.888950	0.375360	0.001011	0.719601
-4.435629	-1.891239	0.380365	0.001006	0.719605
-4.821958	-1.970739	0.385370	0.001078	0.719314
-5.514400	-1.870920	0.390374	0.001207	0.719268
-5.652893	-1.841693	0.395379	0.001232	0.719277
-5.223346	-1.921468	0.400384	0.001152	0.719271
-5.420338	-1.973285	0.405389	0.001188	0.719100
-6.385327	-1.871010	0.410394	0.001368	0.718964
-6.364839	-1.878408	0.415398	0.001364	0.718957
-6.093306	-1.923711	0.420403	0.001313	0.718963
-6.045477	-1.932971	0.425408	0.001304	0.718962
-6.834260	-1.936103	0.430413	0.001450	0.718680
-7.176481	-1.891080	0.435418	0.001514	0.718649
-7.261204	-1.879183	0.440422	0.001529	0.718643
-7.038864	-1.916479	0.445427	0.001487	0.718648
-7.468210	-1.842730	0.450432	0.001567	0.718643
-7.554335	-1.909229	0.455437	0.001583	0.718482
-8.065793	-1.880230	0.460442	0.001678	0.718360
-8.091341	-1.879346	0.465446	0.001682	0.718353
-7.944517	-1.901929	0.470451	0.001655	0.718361
-7.762499	-1.935880	0.475456	0.001621	0.718358
-8.193178	-1.862009	0.480461	0.001700	0.718353
-8.501511	-1.961010	0.485466	0.001758	0.718050
-9.071623	-1.876446	0.490470	0.001863	0.718017
-9.148327	-1.859575	0.495475	0.001877	0.718024
-9.169443	-1.859044	0.500480	0.001881	0.718018
-9.004730	-1.889675	0.505485	0.001850	0.718016
-9.026966	-1.881754	0.510490	0.001854	0.718024
-9.537143	-1.909027	0.515494	0.001949	0.717791
-10.401107	-1.796837	0.520499	0.002109	0.717709
-10.056281	-1.860971	0.525504	0.002045	0.717705
-9.966440	-1.878425	0.530509	0.002028	0.717702
-9.951235	-1.877767	0.535514	0.002025	0.717709
-9.692083	-1.928221	0.540518	0.001976	0.717701
-9.657606	-1.957849	0.545523	0.001970	0.717656
-10.890584	-1.876167	0.550528	0.002199	0.717383
-11.131558	-1.836907	0.555533	0.002243	0.717377
-10.769449	-1.898633	0.560538	0.002176	0.717383
-11.131745	-1.837565	0.565542	0.002243	0.717376
-11.081863	-1.844782	0.570547	0.002233	0.717380
-10.930749	-1.872045	0.575552	0.002205	0.717380
-10.812811	-1.914554	0.580557	0.002183	0.717338
-11.631618	-1.894030	0.585562	0.002335	0.717091
-11.739487	-1.880212	0.590566	0.002355	0.717081
-11.922930	-1.845397	0.595571	0.002388	0.717085
-11.862896	-1.859198	0.600576	0.002377	0.717080
-11.849458	-1.863713	0.605581	0.002374	0.717076
-11.596176	-1.904360	0.610586	0.002327	0.717085
-11.946057	-1.881758	0.615590	0.002392	0.717007
-12.771240	-1.860547	0.620595	0.002545	0.716759
-12.370744	-1.933651	0.625600	0.002470	0.716756
-13.037421	-1.818556	0.630605	0.002594	0.716749
-12.731915	-1.867918	0.635610	0.002537	0.716760
-12.622269	-1.892448	0.640614	0.002516	0.716751
-12.508768	-1.909699	0.645619	0.002495	0.716757
-12.751725	-1.915034	0.650624	0.002540	0.716661
-13.947514	-1.810081	0.655629	0.002762	0.716448
-12.941524	-1.985328	0.660634	0.002575	0.716456
-13.548080	-1.882436	0.665638	0.002687	0.716447
-13.717120	-1.850384	0.670643	0.002718	0.716451
-13.679398	-1.857489	0.675648	0.002711	0.716451
-13.826887	-1.833848	0.680653	0.002738	0.716446
-13.769028	-1.871698	0.685658	0.002727	0.716392
-14.574795	-1.860563	0.690662	0.002877	0.716130
-14.455432	-1.879926	0.695667	0.002854	0.716135
-14.778334	-1.822121	0.700672	0.002914	0.716136
-14.729798	-1.833713	0.705677	0.002905	0.716130
-14.187365	-1.925011	0.710682	0.002804	0.716141
-14.848300	-1.814004	0.715686	0.002926	0.716129
-14.721092	-1.830942	0.720691	0.002902	0.716140
-14.493541	-1.956524	0.725696	0.002860	0.715973
-15.589191	-1.805571	0.730701	0.003064	0.715885
-15.358664	-1.843595	0.735706	0.003020	0.715892
-15.528145	-1.819658	0.740710	0.003052	0.715880
-15.194783	-1.875804	0.745715	0.002989	0.715887
-15.182602	-1.878753	0.750720	0.002987	0.715886
-15.694626	-1.789974	0.755725	0.003082	0.715882
-15.452005	-1.969669	0.760730	0.003036	0.715612
-16.060349	-1.896405	0.765734	0.003149	0.715543
-16.463078	-1.821583	0.770739	0.003224	0.715549
-16.302992	-1.850486	0.775744	0.003194	0.715549
-16.506090	-1.815596	0.780749	0.003231	0.715547
-16.083676	-1.888869	0.785754	0.003153	0.715552
-16.569386	-1.807019	0.790758	0.003243	0.715543
-16.808874	-1.895764	0.795763	0.003287	0.715283
-17.083575	-1.871255	0.800768	0.003338	0.715235
-17.506518	-1.798615	0.805773	0.003416	0.715230
-16.982851	-1.886624	0.810778	0.003319	0.715241
-17.466226	-1.804910	0.815782	0.003408	0.715233
-17.211789	-1.848143	0.820787	0.003361	0.715237
-17.252327	-1.842212	0.825792	0.003368	0.715235
-17.487254	-1.897803	0.830797	0.003411	0.715043
-18.252336	-1.825845	0.835802	0.003554	0.714915
-18.419198	-1.800436	0.840806	0.003584	0.714907
-17.996593	-1.872097	0.845811	0.003505	0.714915
-18.029092	-1.867754	0.850816	0.003511	0.714913
-18.533434	-1.781672	0.855821	0.003605	0.714906
-18.084737	-1.857666	0.860826	0.003521	0.714914
-17.992159	-1.905731	0.865830	0.003504	0.714852
-19.116926	-1.826484	0.870835	0.003713	0.714612
-19.130319	-1.825387	0.875840	0.003715	0.714610
-19.429834	-1.773552	0.880845	0.003770	0.714608
-18.888282	-1.866682	0.885850	0.003669	0.714615
-19.381979	-1.783083	0.890854	0.003761	0.714607
-19.283554	-1.799745	0.895859	0.003742	0.714609
-19.038261	-1.841786	0.900864	0.003696	0.714613
-19.448652	-1.872746	0.905869	0.003772	0.714407
-20.337879	-1.775068	0.910874	0.003938	0.714287
-20.055635	-1.832613	0.915878	0.003885	0.714273
-20.208582	-1.802684	0.920883	0.003913	0.714279
-20.297041	-1.788095	0.925888	0.003929	0.714277
-20.068138	-1.830086	0.930893	0.003886	0.714275
-20.231462	-1.797798	0.935898	0.003916	0.714282
-20.693627	-1.719577	0.940902	0.004002	0.714274
-20.107239	-1.926931	0.945907	0.003893	0.714070
-20.703928	-1.871638	0.950912	0.004004	0.713969
-21.203470	-1.784673	0.955917	0.004096	0.713966
-20.731467	-1.864713	0.960922	0.004008	0.713974
-21.025264	-1.817742	0.965926	0.004063	0.713964
-21.125371	-1.795892	0.970931	0.004081	0.713973
-20.995870	-1.819585	0.975936	0.004057	0.713972
-21.348164	-1.861463	0.980941	0.004122	0.713765
-21.754395	-1.844475	0.985946	0.004197	0.713655
-21.866889	-1.827486	0.990950	0.004218	0.713650
-22.182631	-1.769025	0.995955	0.004276	0.713654
-21.929258	-1.814238	1.000960	0.004229	0.713655
-22.043642	-1.798248	1.005965	0.004250	0.713647
-21.876232	-1.823866	1.010970	0.004219	0.713656
-22.171625	-1.805342	1.015974	0.004273	0.713588
-22.612213	-1.841277	1.020979	0.004355	0.713361
-22.498050	-1.863376	1.025984	0.004334	0.713358
-23.078801	-1.762917	1.030989	0.004441	0.713353
-22.591862	-1.846645	1.035994	0.004350	0.713359
-22.714876	-1.827663	1.040998	0.004373	0.713354
-22.700758	-1.826286	1.046003	0.004370	0.713362
-22.392994	-1.944559	1.051008	0.004313	0.713237
-23.910698	-1.783383	1.056013	0.004595	0.713020
-23.678754	-1.821368	1.061018	0.004551	0.713027
-23.748469	-1.812155	1.066022	0.004564	0.713021
-23.773930	-1.804316	1.071027	0.004569	0.713028
-23.624725	-1.831717	1.076032	0.004541	0.713027
-23.904512	-1.785663	1.081037	0.004592	0.713020
-23.249226	-1.922922	1.086042	0.004470	0.712980
-24.435674	-1.850086	1.091046	0.004691	0.712705
-24.691862	-1.802510	1.096051	0.004738	0.712709
-24.751967	-1.793009	1.101056	0.004749	0.712707
-24.726673	-1.799743	1.106061	0.004744	0.712703
-24.555408	-1.826566	1.111066	0.004712	0.712711
-24.830037	-1.780605	1.116070	0.004763	0.712706
-24.740990	-1.793759	1.121075	0.004746	0.712712
-24.824877	-1.872015	1.126080	0.004761	0.712527
-25.877311	-1.757881	1.131085	0.004957	0.712381
-25.248154	-1.864493	1.136090	0.004839	0.712392
-25.628691	-1.801422	1.141094	0.004910	0.712383
-25.955784	-1.741761	1.146099	0.004971	0.712387
-25.419891	-1.836535	1.151104	0.004871	0.712389
-25.506894	-1.825570	1.156109	0.004887	0.712380
-25.798645	-1.796147	1.161114	0.004941	0.712336
-26.484678	-1.799293	1.166118	0.005068	0.712086
-26.301163	-1.829204	1.171123	0.005034	0.712093
-26.577737	-1.779837	1.176128	0.005085	0.712093
-26.745125	-1.754038	1.181133	0.005116	0.712086
-26.139424	-1.857846	1.186138	0.005003	0.712095
-26.626606	-1.776630	1.191142	0.005093	0.712084
-26.545384	-1.786748	1.196147	0.005078	0.712093
-26.441597	-1.934617	1.201152	0.005058	0.711836
-27.416594	-1.800456	1.206157	0.005239	0.711757
-27.350788	-1.808300	1.211162	0.005227	0.711766
-27.199554	-1.841700	1.216166	0.005198	0.711753
-27.475778	-1.789302	1.221171	0.005249	0.711760
-27.292633	-1.823026	1.226176	0.005215	0.711759
-27.349618	-1.813138	1.231181	0.005225	0.711759
-27.474751	-1.916553	1.236186	0.005249	0.711508
-28.291049	-1.799887	1.241190	0.005400	0.711452
-28.411764	-1.777078	1.246195	0.005422	0.711455
-27.904256	-1.867624	1.251200	0.005328	0.711455
-28.273003	-1.803786	1.256205	0.005396	0.711452
-28.432050	-1.772347	1.261210	0.005425	0.711459
-28.188197	-1.821976	1.266214	0.005380	0.711447
-28.572433	-1.874584	1.271219	0.005451	0.711206
-29.218395	-1.793771	1.276224	0.005571	0.711138
-29.504945	-1.743757	1.281229	0.005624	0.711136
-28.844625	-1.858876	1.286234	0.005501	0.711142
-29.226998	-1.795972	1.291238	0.005572	0.711132
-29.414760	-1.760472	1.296243	0.005606	0.711137
-28.933413	-1.844755	1.301248	0.005516	0.711140
-29.289288	-1.844022	1.306253	0.005582	0.711015
-30.189993	-1.754007	1.311258	0.005750	0.710875
-29.975300	-1.797615	1.316262	0.005710	0.710865
-30.039896	-1.783087	1.321267	0.005721	0.710872
-29.917424	-1.806195	1.326272	0.005698	0.710870
-29.796606	-1.831354	1.331277	0.005676	0.710863
-29.788439	-1.827994	1.336282	0.005674	0.710873
-30.074242	-1.871970	1.341286	0.005727	0.710684
-31.475135	-1.697509	1.346291	0.005987	0.710535
-30.730987	-1.831169	1.351296	0.005848	0.710533
-30.858753	-1.811871	1.356301	0.005872	0.710527
-31.062916	-1.769347	1.361306	0.005910	0.710539
-31.071091	-1.771439	1.366310	0.005911	0.710533
-30.852674	-1.808988	1.371315	0.005870	0.710536
-30.815775	-1.850256	1.376320	0.005863	0.710467
-32.119440	-1.744771	1.381325	0.006105	0.710214
-31.653445	-1.826247	1.386330	0.006018	0.710218
-31.921341	-1.782405	1.391334	0.006068	0.710211
-32.051563	-1.756809	1.396339	0.006092	0.710216
-31.765349	-1.808629	1.401344	0.006038	0.710215
-32.141793	-1.744740	1.406349	0.006108	0.710209
-31.922270	-1.779949	1.411354	0.006067	0.710218
-32.152011	-1.843543	1.416358	0.006109	0.710009
-32.984329	-1.753225	1.421363	0.006264	0.709894
-32.556900	-1.828651	1.426368	0.006184	0.709896
-32.691575	-1.808782	1.431373	0.006209	0.709888
-32.504687	-1.837709	1.436378	0.006174	0.709897
-32.686138	-1.809777	1.441382	0.006207	0.709889
-33.149642	-1.725255	1.446387	0.006293	0.709893
-32.884930	-1.850417	1.451392	0.006244	0.709738
-33.627717	-1.792184	1.456397	0.006382	0.709590
-33.452493	-1.819699	1.461402	0.006349	0.709598
-33.743788	-1.771681	1.466406	0.006403	0.709591
-33.587511	-1.797692	1.471411	0.006374	0.709595
-33.587281	-1.796635	1.476416	0.006373	0.709598
-33.979201	-1.730645	1.481421	0.006446	0.709591
-33.785475	-1.828257	1.486426	0.006410	0.709465
-34.556167	-1.793414	1.491430	0.006553	0.709261
-34.292893	-1.838886	1.496435	0.006504	0.709264
-34.391338	-1.821023	1.501440	0.006522	0.709265
-34.768982	-1.757535	1.506445	0.006592	0.709258
-34.603669	-1.782701	1.511450	0.006561	0.709267
-34.833515	-1.744579	1.516454	0.006603	0.709262
-34.699625	-1.797413	1.521459	0.006578	0.709205
-35.287500	-1.817216	1.526464	0.006687	0.708956
-35.560176	-1.773564	1.531469	0.006737	0.708946
-35.358501	-1.803186	1.536474	0.006700	0.708960
-35.489966	-1.785207	1.541478	0.006724	0.708949
-35.618284	-1.759876	1.546483	0.006747	0.708955
-35.541120	-1.773584	1.551488	0.006733	0.708955
-35.224176	-1.833067	1.556493	0.006674	0.708950
-35.660955	-1.905316	1.561498	0.006755	0.708650
-36.492340	-1.765433	1.566502	0.006909	0.708634
-36.381290	-1.785882	1.571507	0.006888	0.708633
-35.866549	-1.872280	1.576512	0.006792	0.708644
-36.526625	-1.759890	1.581517	0.006915	0.708634
-36.686706	-1.727612	1.586522	0.006944	0.708642
-36.139279	-1.831136	1.591526	0.006842	0.708631
-37.033002	-1.814625	1.596531	0.007008	0.708345
-37.334158	-1.759230	1.601536	0.007064	0.708349
-37.591376	-1.716690	1.606541	0.007111	0.708343
-37.126379	-1.795629	1.611546	0.007025	0.708352
-37.497359	-1.732891	1.616550	0.007093	0.708345
-37.367381	-1.754494	1.621555	0.007069	0.708349
-36.880247	-1.840571	1.626560	0.006978	0.708351
-37.576656	-1.833080	1.631565	0.007107	0.708118
-38.355574	-1.746843	1.636570	0.007252	0.708013
-37.833480	-1.844916	1.641574	0.007155	0.708003
-38.297191	-1.760898	1.646579	0.007241	0.708007
-38.370359	-1.745788	1.651584	0.007254	0.708011
-37.848315	-1.842450	1.656589	0.007157	0.708005
-37.780611	-1.850736	1.661594	0.007144	0.708013
-38.595043	-1.814402	1.666598	0.007295	0.707795
-39.196054	-1.757124	1.671603	0.007407	0.707696
-38.455377	-1.886258	1.676608	0.007269	0.707702
-38.968339	-1.798207	1.681613	0.007364	0.707696
-39.125047	-1.766028	1.686618	0.007393	0.707705
-38.920167	-1.807483	1.691622	0.007354	0.707695
-38.758951	-1.836330	1.696627	0.007324	0.707696
-39.327800	-1.855036	1.701632	0.007430	0.707455
-40.316582	-1.722388	1.706637	0.007613	0.707368
-39.841527	-1.802587	1.711642	0.007525	0.707378
-39.864121	-1.802755	1.716646	0.007529	0.707370
-40.017930	-1.771794	1.721651	0.007557	0.707378
-39.792870	-1.812372	1.726656	0.007515	0.707377
-40.040014	-1.772204	1.731661	0.007560	0.707370
-39.875012	-1.864691	1.736666	0.007530	0.707244
-40.680386	-1.805815	1.741670	0.007679	0.707075
-40.670081	-1.806092	1.746675	0.007677	0.707078
-40.840693	-1.774159	1.751680	0.007708	0.707082
-40.943209	-1.760002	1.756685	0.007727	0.707074
-40.518326	-1.831377	1.761690	0.007648	0.707083
-40.834717	-1.777425	1.766694	0.007707	0.707079
-41.148936	-1.802461	1.771699	0.007765	0.706917
-41.342895	-1.848680	1.776704	0.007801	0.706755
-41.464074	-1.832709	1.781709	0.007823	0.706744
-41.963641	-1.738409	1.786714	0.007916	0.706755
-41.963317	-1.742736	1.791718	0.007915	0.706747
-41.598547	-1.806159	1.796723	0.007847	0.706751
-41.793062	-1.768567	1.801728	0.007883	0.706758
-42.098123	-1.743366	1.806733	0.007939	0.706699
-42.230829	-1.845224	1.811738	0.007964	0.706448
-42.343488	-1.829177	1.816742	0.007985	0.706440
-42.910341	-1.728515	1.821747	0.008090	0.706440
-42.467513	-1.804263	1.826752	0.008007	0.706447
-42.421003	-1.816277	1.831757	0.007998	0.706440
-42.891650	-1.727677	1.836762	0.008086	0.706450
-42.626399	-1.789714	1.841766	0.008036	0.706421
-43.088162	-1.852625	1.846771	0.008122	0.706130
-43.679529	-1.746854	1.851776	0.008231	0.706131
-43.741942	-1.739179	1.856781	0.008243	0.706124
-43.076215	-1.854120	1.861786	0.008119	0.706132
-43.536562	-1.776984	1.866790	0.008204	0.706123
-43.994730	-1.693636	1.871795	0.008289	0.706127
-43.244751	-1.824994	1.876800	0.008149	0.706132
-43.483516	-1.899265	1.881805	0.008193	0.705898
-44.431264	-1.746223	1.886810	0.008369	0.705866
-44.502747	-1.737279	1.891814	0.008382	0.705859
-44.074316	-1.811475	1.896819	0.008302	0.705864
-44.167586	-1.793175	1.901824	0.008320	0.705868
-44.653435	-1.710985	1.906829	0.008410	0.705860
-44.143062	-1.805842	1.911834	0.008314	0.705852
-44.920610	-1.832311	1.916838	0.008459	0.705521
-45.523262	-1.724523	1.921843	0.008571	0.705522
-45.316208	-1.758249	1.926848	0.008532	0.705529
-45.272833	-1.771020	1.931853	0.008524	0.705520
-45.200099	-1.778318	1.936858	0.008510	0.705531
-45.232060	-1.777310	1.941862	0.008516	0.705523
-45.203539	-1.782506	1.946867	0.008510	0.705523
-45.440351	-1.868533	1.951872	0.008554	0.705265
-46.551053	-1.699523	1.956877	0.008760	0.705207
-45.882403	-1.813060	1.961882	0.008636	0.705219
-45.752823	-1.842592	1.966886	0.008611	0.705207
-46.457767	-1.714125	1.971891	0.008742	0.705213
-45.977841	-1.799406	1.976896	0.008652	0.705214
-45.858069	-1.825833	1.981901	0.008630	0.705205
-46.517029	-1.856344	1.986906	0.008752	0.704907
-47.165779	-1.750914	1.991910	0.008873	0.704887
-46.966936	-1.785235	1.996915	0.008835	0.704890
-46.713278	-1.832871	2.001920	0.008788	0.704886

-46.962403	-1.787518	2.011917	0.008834	0.704889
-46.982155	-1.808935	2.021914	0.008837	0.704839
-47.695125	-1.807307	2.031910	0.008969	0.704588
-48.038774	-1.746497	2.041907	0.009033	0.704588
-47.867030	-1.776564	2.051904	0.009000	0.704590
-47.097755	-1.855402	2.061901	0.008856	0.704709
-47.425350	-1.755442	2.071898	0.008917	0.704793
-46.835765	-1.813441	2.081894	0.008806	0.704889
-47.151402	-1.757199	2.091891	0.008865	0.704890
-46.807131	-1.818992	2.101888	0.008800	0.704891
-47.185733	-1.752767	2.111885	0.008870	0.704889
-47.035169	-1.779521	2.121882	0.008841	0.704890
-46.952837	-1.796052	2.131878	0.008825	0.704888
-47.272657	-1.740190	2.141875	0.008884	0.704886
-46.618191	-1.742722	2.151872	0.008762	0.705117
-46.077584	-1.790373	2.161869	0.008661	0.705217
-46.195040	-1.769695	2.171866	0.008682	0.705217
-46.039920	-1.799707	2.181862	0.008653	0.705213
-46.517353	-1.685973	2.191859	0.008741	0.705272
-45.110910	-1.812471	2.201856	0.008478	0.705523
-45.398594	-1.761953	2.211853	0.008531	0.705523
-45.077214	-1.819856	2.221850	0.008471	0.705523
-45.152519	-1.807470	2.231846	0.008485	0.705522
-44.406651	-1.775361	2.241843	0.008345	0.705855
-44.368258	-1.780562	2.251840	0.008337	0.705859
-44.353206	-1.783391	2.261837	0.008334	0.705860
-44.378115	-1.772334	2.271834	0.008338	0.705874
-43.699915	-1.768386	2.281830	0.008211	0.706126
-43.676679	-1.774072	2.291827	0.008206	0.706124
-43.360204	-1.830088	2.301824	0.008147	0.706126
-43.479110	-1.734238	2.311821	0.008168	0.706277
-42.429809	-1.838757	2.321818	0.007973	0.706444
-42.818800	-1.770534	2.331814	0.008044	0.706443
-42.895105	-1.755326	2.341811	0.008058	0.706447
-42.135580	-1.741058	2.351808	0.007916	0.706749
-41.962368	-1.770638	2.361805	0.007883	0.706753
-41.905427	-1.780154	2.371802	0.007872	0.706755
-41.480147	-1.744614	2.381798	0.007792	0.706980
-41.193480	-1.745995	2.391795	0.007738	0.707081
-40.928428	-1.792878	2.401792	0.007689	0.707083
-41.132294	-1.718960	2.411789	0.007726	0.707159
-40.090026	-1.795469	2.421786	0.007531	0.707379
-40.435036	-1.735791	2.431782	0.007595	0.707377
-40.177651	-1.782670	2.441779	0.007547	0.707376
-39.670330	-1.737102	2.451776	0.007451	0.707650
-39.487299	-1.744662	2.461773	0.007417	0.707701
-39.230375	-1.791028	2.471770	0.007368	0.707701
-39.182579	-1.730213	2.481766	0.007359	0.707841
-38.337622	-1.797006	2.491763	0.007201	0.708010
-38.368656	-1.791423	2.501760	0.007206	0.708011
-38.477042	-1.770728	2.511757	0.007226	0.708015
-37.795469	-1.749924	2.521754	0.007098	0.708302
-37.732328	-1.737727	2.531750	0.007086	0.708350
-37.436767	-1.790822	2.541747	0.007031	0.708350
-37.306261	-1.774169	2.551744	0.007006	0.708431
-36.646607	-1.789089	2.561741	0.006882	0.708638
-36.336989	-1.844181	2.571738	0.006824	0.708639
-36.806917	-1.762208	2.581734	0.006911	0.708636
-36.146078	-1.768212	2.591731	0.006787	0.708861
-36.056399	-1.738396	2.601728	0.006770	0.708954
-35.712216	-1.800116	2.611725	0.006706	0.708954
-35.687065	-1.752430	2.621722	0.006700	0.709060
-34.878941	-1.794998	2.631718	0.006549	0.709264
-34.912762	-1.791339	2.641715	0.006555	0.709260
-35.110586	-1.755561	2.651712	0.006591	0.709262
-34.215486	-1.769998	2.661709	0.006424	0.709554
-34.145779	-1.760957	2.671706	0.006411	0.709598
-34.206565	-1.751126	2.681702	0.006421	0.709597
-33.991020	-1.724113	2.691699	0.006381	0.709729
-33.325127	-1.760341	2.701696	0.006256	0.709895
-33.237458	-1.776498	2.711693	0.006239	0.709895
-33.333417	-1.738821	2.721690	0.006257	0.709937
-32.598240	-1.728986	2.731686	0.006119	0.710219
-32.321707	-1.779934	2.741683	0.006067	0.710217
-32.687709	-1.715438	2.751680	0.006135	0.710217
-31.970866	-1.715420	2.761677	0.006001	0.710473
-31.335735	-1.799951	2.771674	0.005882	0.710531
-31.709773	-1.731911	2.781670	0.005951	0.710535
-31.397268	-1.741493	2.791667	0.005892	0.710628
-30.713957	-1.743012	2.801664	0.005764	0.710870
-30.606051	-1.759838	2.811661	0.005744	0.710875
-30.833406	-1.719348	2.821658	0.005785	0.710876
-29.953917	-1.755349	2.831654	0.005621	0.711118
-30.003596	-1.736612	2.841651	0.005630	0.711139
-29.871932	-1.759668	2.851648	0.005605	0.711141
-29.735068	-1.700814	2.861645	0.005579	0.711308
-28.931050	-1.770225	2.871642	0.005428	0.711457
-29.356098	-1.695017	2.881638	0.005507	0.711457
-28.732499	-1.787865	2.891635	0.005390	0.711494
-28.529011	-1.690474	2.901632	0.005352	0.711762
-28.118364	-1.764024	2.911629	0.005275	0.711762
-28.374478	-1.718253	2.921626	0.005322	0.711763
-27.508494	-1.723878	2.931622	0.005160	0.712061
-27.320891	-1.742545	2.941619	0.005125	0.712091
-27.295101	-1.748341	2.951616	0.005119	0.712090
-27.107641	-1.724428	2.961613	0.005084	0.712205
-26.277323	-1.782136	2.971610	0.004929	0.712386
-26.516614	-1.739444	2.981606	0.004973	0.712387
-26.534294	-1.737964	2.991603	0.004975	0.712385
-25.915329	-1.699353	3.001600	0.004860	0.712683
-25.307010	-1.793321	3.011597	0.004746	0.712712
-25.721706	-1.721966	3.021594	0.004822	0.712708
-25.204698	-1.744429	3.031590	0.004726	0.712848
-24.694750	-1.749126	3.041587	0.004630	0.713021
-24.771673	-1.735050	3.051584	0.004644	0.713023
-24.919008	-1.700771	3.061581	0.004671	0.713040
-23.872932	-1.725577	3.071578	0.004475	0.713362
-23.714578	-1.753617	3.081574	0.004445	0.713364
-23.954061	-1.713603	3.091571	0.004489	0.713359
-23.641540	-1.690719	3.101568	0.004431	0.713517
-22.684471	-1.793463	3.111565	0.004252	0.713652
-23.164146	-1.709360	3.121562	0.004341	0.713651
-22.901027	-1.746395	3.131558	0.004291	0.713671
-22.301757	-1.705633	3.141555	0.004179	0.713966
-21.844320	-1.787468	3.151552	0.004093	0.713966
-22.083069	-1.743341	3.161549	0.004137	0.713970
-21.738123	-1.717271	3.171546	0.004072	0.714145
-21.088350	-1.766771	3.181542	0.003951	0.714278
-21.286494	-1.732829	3.191539	0.003987	0.714276
-21.036898	-1.778302	3.201536	0.003940	0.714275
-20.299556	-1.745234	3.211533	0.003802	0.714603
-20.173691	-1.764412	3.221530	0.003778	0.714611
-20.001403	-1.796112	3.231526	0.003746	0.714610
-20.283598	-1.712242	3.241523	0.003798	0.714677
-19.349090	-1.764924	3.251520	0.003623	0.714904
-19.368252	-1.760744	3.261517	0.003626	0.714907
-19.431703	-1.749225	3.271514	0.003637	0.714908
-18.509114	-1.783392	3.281510	0.003465	0.715168
-18.599106	-1.736574	3.291507	0.003481	0.715230
-18.571447	-1.739868	3.301504	0.003476	0.715234
-18.423842	-1.720637	3.311501	0.003447	0.715326
-17.424323	-1.786675	3.321498	0.003261	0.715549
-17.703267	-1.738856	3.331494	0.003312	0.715546
-17.704779	-1.740618	3.341491	0.003312	0.715543
-17.068679	-1.723622	3.351488	0.003193	0.715802
-16.769281	-1.737386	3.361485	0.003137	0.715882
-16.525365	-1.780187	3.371482	0.003091	0.715884
-16.518792	-1.769350	3.381478	0.003089	0.715909
-16.398048	-1.680084	3.391475	0.003066	0.716130
-15.800801	-1.787284	3.401472	0.002954	0.716129
-16.094852	-1.734490	3.411469	0.003008	0.716131
-15.110736	-1.763109	3.421466	0.002824	0.716423
-14.890254	-1.789419	3.431462	0.002783	0.716449
-14.836909	-1.800126	3.441459	0.002772	0.716448
-14.653497	-1.813043	3.451456	0.002738	0.716488
-14.021699	-1.790352	3.461453	0.002619	0.716757
-13.676589	-1.852319	3.471450	0.002555	0.716757
-13.833003	-1.826215	3.481446	0.002583	0.716755
-13.862022	-1.776601	3.491443	0.002588	0.716844
-12.576029	-1.886365	3.501440	0.002348	0.717081
-12.807983	-1.844436	3.511437	0.002391	0.717083
-12.583970	-1.884041	3.521434	0.002348	0.717085
-12.798333	-1.810795	3.531430	0.002388	0.717155
-11.915842	-1.855859	3.541427	0.002223	0.717378
-12.006902	-1.840410	3.551424	0.002239	0.717377
-11.962069	-1.846953	3.561421	0.002230	0.717381
-11.542842	-1.837372	3.571418	0.002152	0.717549
-10.828081	-1.887645	3.581414	0.002018	0.717702
-10.968597	-1.863348	3.591411	0.002044	0.717702
-10.890586	-1.878606	3.601408	0.002029	0.717700
-10.589633	-1.828656	3.611405	0.001972	0.717906
-10.026822	-1.870771	3.621402	0.001867	0.718022
-10.187273	-1.843754	3.631398	0.001896	0.718020
-9.916446	-1.893712	3.641395	0.001845	0.718017
-9.608069	-1.779934	3.651392	0.001787	0.718352
-9.100376	-1.869585	3.661389	0.001692	0.718354
-9.065209	-1.875748	3.671386	0.001685	0.718355
-9.014089	-1.821183	3.681382	0.001675	0.718482
-8.143648	-1.895902	3.691379	0.001512	0.718642
-8.407969	-1.850427	3.701376	0.001561	0.718640
-8.431015	-1.844995	3.711373	0.001565	0.718643
-7.500771	-1.875486	3.721370	0.001391	0.718911
-7.593155	-1.832906	3.731366	0.001407	0.718964
-7.332994	-1.880249	3.741363	0.001358	0.718963
-7.616935	-1.785644	3.751360	0.001411	0.719051
-6.469904	-1.878519	3.761357	0.001197	0.719272
-6.539577	-1.866683	3.771354	0.001209	0.719271
-6.543339	-1.868686	3.781350	0.001209	0.719267
-5.900015	-1.858732	3.791347	0.001089	0.719514
-5.684823	-1.852588	3.801344	0.001048	0.719603
-5.613869	-1.866313	3.811341	0.001034	0.719601
-5.499007	-1.873106	3.821338	0.001013	0.719629
-4.895638	-1.844582	3.831334	0.000900	0.719898
-4.668634	-1.886574	3.841331	0.000857	0.719896
-4.727312	-1.878442	3.851328	0.000867	0.719893
-4.490751	-1.843981	3.861325	0.000823	0.720045
-3.851828	-1.868537	3.871322	0.000703	0.720222
-3.761559	-1.884708	3.881318	0.000686	0.720222
-3.834559	-1.872122	3.891315	0.000699	0.720223
-3.359690	-1.808205	3.901312	0.000610	0.720516
-3.042058	-1.852676	3.911309	0.000550	0.720541
-3.027400	-1.854985	3.921306	0.000547	0.720543
-2.683931	-1.833848	3.931302	0.000482	0.720706
-2.772389	-1.728664	3.941299	0.000498	0.720883
-2.354044	-1.804926	3.951296	0.000420	0.720880
-2.436659	-1.736321	3.961293	0.000434	0.720987
-1.952950	-1.754766	3.971290	0.000344	0.721121
-2.194346	-1.712630	3.981286	0.000388	0.721121
-1.878916	-1.660672	3.991283	0.000329	0.721334
-1.856334	-1.613826	4.001280	0.000324	0.721435
-1.666565	-1.610103	4.011277	0.000288	0.721510
-1.536872	-1.515981	4.021274	0.000263	0.721742
-1.284945	-1.559862	4.031270	0.000216	0.721745
-1.246233	-1.408440	4.041267	0.000208	0.722057
-1.235238	-1.403052	4.051264	0.000205	0.722072
-1.255483	-1.264864	4.061261	0.000209	0.722337
-1.068588	-1.278094	4.071258	0.000173	0.722378
-0.906777	-1.148330	4.081254	0.000142	0.722690
-0.523051	-1.188112	4.091251	0.000071	0.722747
-0.438031	-1.075072	4.101248	0.000054	0.723000
-0.612762	-0.968865	4.111245	0.000086	0.723148
-0.565844	-0.880142	4.121242	0.000077	0.723339
-0.685143	-0.730460	4.131238	0.000098	0.723592
-0.524821	-0.671999	4.141235	0.000068	0.723764
-0.647435	-0.546786	4.151232	0.000090	0.723967
-0.391172	-0.444858	4.161229	0.000042	0.724257
-0.124657	-0.369648	4.171226	-0.000009	0.724499
-0.134325	-0.256969	4.181222	-0.000007	0.724717
-0.074461	-0.158712	4.191219	-0.000019	0.724931
-0.045159	-0.020933	4.201216	-0.000025	0.725212
-0.027944	0.126210	4.211213	-0.000029	0.725506
0.000000	0.273892	4.221210	-0.000035	0.725806

0.099493	0.881214	4.226214	-0.000054	0.727026
0.145869	2.155514	4.231219	-0.000064	0.729524
0.408427	3.975360	4.236224	-0.000114	0.733144
0.691536	6.344948	4.241229	-0.000169	0.737811
0.957598	9.234212	4.246234	-0.000221	0.743434
1.135500	12.620327	4.251238	-0.000256	0.749925
1.613612	16.396287	4.256243	-0.000348	0.757191
2.006977	20.604490	4.261248	-0.000424	0.765161
2.088035	25.267225	4.266253	-0.000443	0.773781
2.696243	30.201903	4.271258	-0.000559	0.782968
2.995006	35.537458	4.276262	-0.000619	0.792667
3.415262	41.168020	4.281267	-0.000701	0.802808
4.031058	47.076199	4.286272	-0.000820	0.813367
4.307827	53.308951	4.291277	-0.000876	0.824246
4.671805	59.823939	4.296282	-0.000948	0.835488
5.148025	66.508835	4.301286	-0.001041	0.846898
5.423999	73.466735	4.306291	-0.001097	0.858549
5.833900	80.602768	4.311296	-0.001179	0.870373
6.409401	87.881124	4.316301	-0.001291	0.882313
7.381428	95.288993	4.321306	-0.001477	0.894409
7.985363	102.902663	4.326310	-0.001595	0.906564
8.361355	110.710307	4.331315	-0.001670	0.918796
8.884784	118.600169	4.336320	-0.001773	0.931031
9.531648	126.580783	4.341325	-0.001899	0.943276
10.195925	134.685211	4.346330	-0.002028	0.955552
10.760691	142.865415	4.351334	-0.002139	0.967757
13.826229	150.731317	4.356339	-0.002715	0.979986
14.351100	159.165662	4.361344	-0.002819	0.992243
15.010215	167.589509	4.366349	-0.002947	1.004368
15.308742	176.132474	4.371354	-0.003009	1.016426
16.120225	184.607441	4.376358	-0.003165	1.028372
16.894313	193.138420	4.381363	-0.003315	1.040248
17.853418	201.669892	4.386368	-0.003500	1.052033
18.704496	210.243231	4.391373	-0.003664	1.063718
19.377721	218.896784	4.396378	-0.003795	1.075341
20.140969	227.495094	4.401382	-0.003943	1.086787
20.715883	236.157658	4.406387	-0.004056	1.098155
21.413303	244.803267	4.411392	-0.004192	1.109411
21.927634	253.468214	4.416397	-0.004294	1.120538
22.659568	262.105261	4.421402	-0.004436	1.131567
23.097251	270.778979	4.426406	-0.004524	1.142472
23.760364	279.439974	4.431411	-0.004653	1.153306
24.651367	288.028503	4.436416	-0.004825	1.163998
25.302244	296.637202	4.441421	-0.004952	1.174567
26.249282	305.202372	4.446426	-0.005134	1.185050
26.661019	313.848851	4.451430	-0.005217	1.195428
27.216582	322.434691	4.456435	-0.005326	1.205675
28.110647	330.983903	4.461440	-0.005498	1.215859
28.801427	339.534844	4.466445	-0.005633	1.225920
29.439928	348.127856	4.471450	-0.005757	1.235937
30.046836	356.654709	4.476454	-0.005876	1.245792
30.828595	365.173079	4.481459	-0.006028	1.255593
31.538713	373.677936	4.486464	-0.006166	1.265289
31.891770	382.240224	4.491469	-0.006237	1.274908
32.554852	390.716895	4.496474	-0.006367	1.284418
32.728942	399.272394	4.501478	-0.006405	1.293854
33.338791	407.724616	4.506483	-0.006524	1.303189
34.051955	416.250690	4.511488	-0.006663	1.312555
34.585090	424.711818	4.516493	-0.006768	1.321753
34.934045	433.158373	4.521498	-0.006839	1.330839
35.677749	441.521232	4.526502	-0.006983	1.339844
36.298885	449.906910	4.531507	-0.007104	1.348792
36.792258	458.325721	4.536512	-0.007202	1.357692
37.350137	466.683912	4.541517	-0.007311	1.366482
38.167540	475.038241	4.546522	-0.007469	1.375257
38.479356	483.444680	4.551526	-0.007533	1.383943
38.762373	491.859577	4.556531	-0.007592	1.392578
39.297954	500.202762	4.561536	-0.007697	1.401130
39.599759	508.562268	4.566541	-0.007759	1.409607
40.031933	516.913415	4.571546	-0.007845	1.418047
40.374207	525.245316	4.576550	-0.007915	1.426402
41.031581	533.550788	4.581555	-0.008043	1.434734
41.595526	541.851612	4.586560	-0.008153	1.442998
41.721746	550.201927	4.591565	-0.008183	1.451193
42.320101	558.490898	4.596570	-0.008300	1.459357
42.925710	566.766639	4.601574	-0.008418	1.467464
43.437602	575.111560	4.606579	-0.008519	1.475578
44.005175	583.368327	4.611584	-0.008631	1.483572
44.174546	591.684467	4.616589	-0.008668	1.491517
44.622797	599.961519	4.621594	-0.008757	1.499427
45.355686	608.168376	4.626598	-0.008899	1.507272
45.633254	616.474832	4.631603	-0.008956	1.515100
46.139440	624.720664	4.636608	-0.009056	1.522866
46.713947	632.942517	4.641613	-0.009169	1.530580
47.594273	641.146971	4.646618	-0.009338	1.538286
48.004678	649.398527	4.651622	-0.009421	1.545926
48.139557	657.737469	4.656627	-0.009451	1.553567
48.656819	665.949505	4.661632	-0.009553	1.561111
49.121759	674.166491	4.666637	-0.009646	1.568616
49.635897	682.405777	4.671642	-0.009747	1.576112
50.072264	690.628375	4.676646	-0.009834	1.583547
50.418959	698.875861	4.681651	-0.009904	1.590956
50.920193	707.093016	4.686656	-0.010003	1.598325
50.925325	715.363615	4.691661	-0.010010	1.605638
51.686451	723.536522	4.696666	-0.010157	1.612937
52.440355	731.691738	4.701670	-0.010303	1.620188
52.807749	739.919847	4.706675	-0.010377	1.627415
53.206067	748.197719	4.711680	-0.010457	1.634658
53.536789	756.379164	4.716685	-0.010524	1.641776
54.004698	764.570307	4.721690	-0.010617	1.648890
54.386674	772.775288	4.726694	-0.010693	1.655973
54.790017	780.951424	4.731699	-0.010774	1.663005
55.339633	789.127276	4.736704	-0.010882	1.670027
55.654032	797.337390	4.741709	-0.010946	1.677016
55.997850	805.523829	4.746714	-0.011016	1.683960
56.468602	813.699601	4.751718	-0.011109	1.690883
56.666068	821.914603	4.756723	-0.011152	1.697775
57.093964	830.087415	4.761728	-0.011237	1.704634
57.606231	838.256565	4.766733	-0.011338	1.711473
58.420470	846.397044	4.771738	-0.011495	1.718300
58.565692	854.577611	4.776742	-0.011528	1.725047
58.936913	862.758163	4.781747	-0.011602	1.731796
59.282771	870.939947	4.786752	-0.011672	1.738517
59.697467	879.064884	4.791757	-0.011755	1.745174
60.075549	887.248465	4.796762	-0.011831	1.751849
60.413344	895.413160	4.801766	-0.011900	1.758478
60.844242	903.546252	4.806771	-0.011986	1.765068
61.539910	911.678134	4.811776	-0.012121	1.771666
61.905206	919.846966	4.816781	-0.012194	1.778227
62.420891	927.986785	4.821786	-0.012296	1.784760
62.548010	936.221417	4.826790	-0.012325	1.791296
62.872811	944.399347	4.831795	-0.012391	1.797787
63.426888	952.504052	4.836800	-0.012500	1.804226
63.613618	960.661124	4.841805	-0.012540	1.810638
64.374283	968.757700	4.846810	-0.012688	1.817049
64.519091	976.921895	4.851814	-0.012720	1.823416
64.670780	985.095982	4.856819	-0.012754	1.829770
65.027848	993.242971	4.861824	-0.012826	1.836104
65.539755	1001.324179	4.866829	-0.012927	1.842385
65.894737	1009.483431	4.871834	-0.012999	1.848686
66.168559	1017.639743	4.876838	-0.013055	1.854953
66.366401	1025.786498	4.881843	-0.013098	1.861183
66.913554	1033.895021	4.886848	-0.013205	1.867403
67.507942	1042.022660	4.891853	-0.013321	1.873623
67.965736	1050.135676	4.896858	-0.013412	1.879795
68.136438	1058.280194	4.901862	-0.013450	1.885938
68.644958	1066.397375	4.906867	-0.013550	1.892079
69.234918	1074.513553	4.911872	-0.013665	1.898208
69.237097	1082.675503	4.916877	-0.013671	1.904285
69.737091	1090.795960	4.921882	-0.013770	1.910368
69.928191	1098.948906	4.926886	-0.013811	1.916420
70.320408	1107.044228	4.931891	-0.013890	1.922434
70.563588	1115.184558	4.936896	-0.013940	1.928445
70.772771	1123.311485	4.941901	-0.013985	1.934424
71.065657	1131.427202	4.946906	-0.014045	1.940386
71.474673	1139.530312	4.951910	-0.014127	1.946332
71.800742	1147.690190	4.956915	-0.014193	1.952293
72.152380	1155.814894	4.961920	-0.014264	1.958212
72.476070	1163.889189	4.966925	-0.014330	1.964075
72.769340	1171.996362	4.971930	-0.014390	1.969940
73.143640	1180.100182	4.976934	-0.014465	1.975794
73.300102	1188.229813	4.981939	-0.014500	1.981626
74.021943	1196.277452	4.986944	-0.014640	1.987442
74.425585	1204.383189	4.991949	-0.014721	1.993248
74.562935	1212.531735	4.996954	-0.014752	1.999040
74.890426	1220.620351	5.001958	-0.014818	2.004793
75.596164	1228.665388	5.006963	-0.014955	2.010538
76.227641	1236.776378	5.011968	-0.015079	2.016305
76.442809	1244.884740	5.016973	-0.015124	2.022010
76.967745	1252.982589	5.021978	-0.015227	2.027724
77.108662	1261.161639	5.026982	-0.015259	2.033439
77.433982	1269.249212	5.031987	-0.015325	2.039093
77.839333	1277.327232	5.036992	-0.015406	2.044733
77.929724	1285.462123	5.041997	-0.015429	2.050365
78.225409	1293.569889	5.047002	-0.015490	2.055983
78.580901	1301.652222	5.052006	-0.015561	2.061574
78.754393	1309.766748	5.057011	-0.015599	2.067154
79.113730	1317.873721	5.062016	-0.015672	2.072732
79.432753	1325.964006	5.067021	-0.015737	2.078280
79.748562	1334.038717	5.072026	-0.015801	2.083802
79.947570	1342.164765	5.077030	-0.015844	2.089333
80.488946	1350.224927	5.082035	-0.015950	2.094838
80.882583	1358.320268	5.087040	-0.016029	2.100338
81.306170	1366.384495	5.092045	-0.016113	2.105805
81.806070	1374.527937	5.097050	-0.016212	2.111318
82.103858	1382.665500	5.102054	-0.016273	2.116794
82.487489	1390.704542	5.107059	-0.016350	2.122198
82.701483	1398.800540	5.112064	-0.016395	2.127609
83.082174	1406.876659	5.117069	-0.016472	2.133010
83.419295	1414.964474	5.122074	-0.016540	2.138401
83.669711	1423.051105	5.127078	-0.016592	2.143768
83.954231	1431.132226	5.132083	-0.016651	2.149122
84.628795	1439.202681	5.137088	-0.016782	2.154492
84.848408	1447.259626	5.142093	-0.016828	2.159798
85.203914	1455.354927	5.147098	-0.016900	2.165128
85.756079	1463.431201	5.152102	-0.017008	2.170450
86.088314	1471.522992	5.157107	-0.017076	2.175749
86.394577	1479.621374	5.162112	-0.017138	2.181037
86.724799	1487.698625	5.167117	-0.017205	2.186301
87.096328	1495.825299	5.172122	-0.017280	2.191588
87.332789	1503.918751	5.177126	-0.017330	2.196828
87.549607	1511.988083	5.182131	-0.017376	2.202038
87.916791	1520.066700	5.187136	-0.017449	2.207256
87.974730	1528.177015	5.192141	-0.017466	2.212453
88.532121	1536.227171	5.197146	-0.017575	2.217645
88.856330	1544.278584	5.202150	-0.017641	2.222804
89.419661	1552.327221	5.207155	-0.017751	2.227971
89.842723	1560.429143	5.212160	-0.017836	2.233147
89.945395	1568.530274	5.217165	-0.017860	2.238282
90.353106	1576.582995	5.222170	-0.017942	2.243402
90.620094	1584.671062	5.227174	-0.017997	2.248520
90.940343	1592.770593	5.232179	-0.018062	2.253638
91.404198	1600.828682	5.237184	-0.018154	2.258731
91.454467	1608.918511	5.242189	-0.018169	2.263796
91.630376	1617.021607	5.247194	-0.018207	2.268869
91.979627	1625.169665	5.252198	-0.018278	2.273974
92.326465	1633.200315	5.257203	-0.018348	2.278994
92.624575	1641.253134	5.262208	-0.018409	2.284013
92.801303	1649.315109	5.267213	-0.018448	2.289015
93.513994	1657.355243	5.272218	-0.018586	2.294039
93.713023	1665.437955	5.277222	-0.018628	2.299034
93.981441	1673.482340	5.282227	-0.018684	2.304001
94.166565	1681.592903	5.287232	-0.018724	2.308991
94.499182	1689.663678	5.292237	-0.018791	2.313958
94.692675	1697.729850	5.297242	-0.018833	2.318899
94.801251	1705.805731	5.302246	-0.018859	2.323829
95.139411	1713.864471	5.307251	-0.018927	2.328757
95.621004	1721.937229	5.312256	-0.019023	2.333695
95.863004	1729.993917	5.317261	-0.019073	2.338593
96.016462	1738.079948	5.322266	-0.019107	2.343491
96.388523	1746.123581	5.327270	-0.019182	2.348371
96.747655	1754.223359	5.332275	-0.019254	2.353274
97.199274	1762.265323	5.337280	-0.019344	2.358139
97.403148	1770.310958	5.342285	-0.019388	2.362976
97.932574	1778.360722	5.347290	-0.019492	2.367832
98.249176	1786.437158	5.352294	-0.019556	2.372677
98.593154	1794.493583	5.357299	-0.019626	2.377502
98.979127	1802.550201	5.362304	-0.019703	2.382321
99.190462	1810.627297	5.367309	-0.019748	2.387128
99.598858	1818.720340	5.372314	-0.019830	2.391950
99.720572	1826.816968	5.377318	-0.019858	2.396743
99.773306	1834.868849	5.382323	-0.019873	2.401493
99.983108	1842.946081	5.387328	-0.019918	2.406262
100.404247	1850.987165	5.392333	-0.020002	2.411016
100.596320	1859.073758	5.397338	-0.020043	2.415770
100.676416	1867.146645	5.402342	-0.020063	2.420498
101.085746	1875.163684	5.407347	-0.020145	2.425209
101.477636	1883.256830	5.412352	-0.020224	2.429954
101.917924	1891.362363	5.417357	-0.020311	2.434700
102.052439	1899.414988	5.422362	-0.020342	2.439383
102.369792	1907.426749	5.427366	-0.020406	2.444048
102.755845	1915.455004	5.432371	-0.020484	2.448718
103.198420	1923.532052	5.437376	-0.020572	2.453412
103.413033	1931.585810	5.442381	-0.020617	2.458066
103.689555	1939.646337	5.447386	-0.020674	2.462719
103.838571	1947.717710	5.452390	-0.020708	2.467361
104.303142	1955.764047	5.457395	-0.020800	2.472003
104.714388	1963.832488	5.462400	-0.020882	2.476645
104.759447	1971.897123	5.467405	-0.020896	2.481248
105.028661	1979.957275	5.472410	-0.020951	2.485857
105.418793	1988.013866	5.477414	-0.021029	2.490465
105.569967	1996.093707	5.482419	-0.021063	2.495059
105.878208	2004.145342	5.487424	-0.021126	2.499641
106.027309	2012.199870	5.492429	-0.021159	2.504204
106.363042	2020.289735	5.497434	-0.021227	2.508792
106.783821	2028.351501	5.502438	-0.021311	2.513362
106.913480	2036.403073	5.507443	-0.021341	2.517897
107.306263	2044.435776	5.512448	-0.021420	2.522433
107.383394	2052.480101	5.517453	-0.021440	2.526943
107.727942	2060.528972	5.522458	-0.021509	2.531468
107.961246	2068.609473	5.527462	-0.021558	2.535994
108.262713	2076.627716	5.532467	-0.021620	2.540482
108.617713	2084.658016	5.537472	-0.021691	2.544972
108.947445	2092.710724	5.542477	-0.021758	2.549466
109.289077	2100.787903	5.547482	-0.021828	2.553965
109.559790	2108.850400	5.552486	-0.021883	2.558444
109.672522	2116.895406	5.557491	-0.021910	2.562894
110.086691	2124.940771	5.562496	-0.021993	2.567357
110.205196	2133.012988	5.567501	-0.022020	2.571807
110.373691	2141.099516	5.572506	-0.022057	2.576260
110.765964	2149.120721	5.577510	-0.022136	2.580685
111.138178	2157.139338	5.582515	-0.022211	2.585100
111.561811	2165.205195	5.587520	-0.022295	2.589537
111.928128	2173.441837	5.592525	-0.022369	2.594055
112.394234	2181.427545	5.597530	-0.022461	2.598435
112.528004	2189.453822	5.602534	-0.022491	2.602807
112.726996	2197.460804	5.607539	-0.022534	2.607166
113.152150	2205.511436	5.612544	-0.022619	2.611557
113.425866	2213.550203	5.617549	-0.022675	2.615923
113.658200	2221.574722	5.622554	-0.022724	2.620272
113.864450	2229.630148	5.627558	-0.022768	2.624628
113.870879	2237.691274	5.632563	-0.022775	2.628967
114.198087	2245.765112	5.637568	-0.022841	2.633327
114.364781	2253.797165	5.642573	-0.022878	2.637646
114.537642	2261.826272	5.647578	-0.022915	2.641957
114.664063	2269.882198	5.652582	-0.022944	2.646273
114.972786	2277.915835	5.657587	-0.023007	2.650581
115.637638	2285.963701	5.662592	-0.023137	2.654913
115.602958	2294.021930	5.667597	-0.023136	2.659198
115.761731	2302.075422	5.672602	-0.023171	2.663486
116.068305	2310.123988	5.677606	-0.023234	2.667774
116.554597	2318.150850	5.682611	-0.023330	2.672056
116.861281	2326.242838	5.687616	-0.023392	2.676353
116.787488	2334.282254	5.692621	-0.023384	2.680591
117.220853	2342.288385	5.697626	-0.023470	2.684837
117.274452	2350.368197	5.702630	-0.023486	2.689091
117.480407	2358.418071	5.707635	-0.023530	2.693332
117.884933	2366.460418	5.712640	-0.023610	2.697575
118.169147	2374.478820	5.717645	-0.023669	2.701792
118.298606	2382.554204	5.722650	-0.023698	2.706021
118.634710	2390.601371	5.727654	-0.023767	2.710243
118.785643	2398.667862	5.732659	-0.023800	2.714456
119.095455	2406.704578	5.737664	-0.023863	2.718657
119.389387	2414.716113	5.742669	-0.023924	2.722837
119.775539	2422.727347	5.747674	-0.024001	2.727017
119.947747	2430.822993	5.752678	-0.024039	2.731220
120.149593	2438.882989	5.757683	-0.024082	2.735400
120.601981	2446.903358	5.762688	-0.024172	2.739569
120.644628	2454.961053	5.767693	-0.024185	2.743726
120.754345	2463.025506	5.772698	-0.024211	2.747884
121.157233	2471.093813	5.777702	-0.024292	2.752055
121.379798	2479.155038	5.782707	-0.024339	2.756205
121.610216	2487.191651	5.787712	-0.024387	2.760337
121.734785	2495.185694	5.792717	-0.024416	2.764435
122.122465	2503.231796	5.797722	-0.024493	2.768569
122.574131	2511.248983	5.802726	-0.024583	2.772686
122.538624	2519.303944	5.807731	-0.024582	2.776786
122.827376	2527.347135	5.812736	-0.024641	2.780894
123.173584	2535.352024	5.817741	-0.024711	2.784980
123.348241	2543.433162	5.822746	-0.024749	2.789088
123.604353	2551.501449	5.827750	-0.024802	2.793189
123.822024	2559.520076	5.832755	-0.024848	2.797256
124.240813	2567.543965	5.837760	-0.024932	2.801331
124.321292	2575.571099	5.842765	-0.024952	2.805383
124.683084	2583.622172	5.847770	-0.025025	2.809456
124.989850	2591.690847	5.852774	-0.025088	2.813530
125.145480	2599.732727	5.857779	-0.025122	2.817576
125.387176	2607.784499	5.862784	-0.025173	2.821625
125.528990	2615.813838	5.867789	-0.025205	2.825652
125.694195	2623.882054	5.872794	-0.025241	2.829694
126.052422	2631.948661	5.877798	-0.025313	2.833740
126.359185	2639.946973	5.882803	-0.025376	2.837743
126.575758	2647.990862	5.887808	-0.025422	2.841758
126.546797	2656.035757	5.892813	-0.025422	2.845754
126.769420	2664.061574	5.897818	-0.025469	2.849750
127.257059	2672.096567	5.902822	-0.025565	2.853759
127.407594	2680.138244	5.907827	-0.025599	2.857746
127.878605	2688.174742	5.912832	-0.025692	2.861744
127.778816	2696.231219	5.917837	-0.025679	2.865714
128.153921	2704.265796	5.922842	-0.025754	2.869694
128.245154	2712.356888	5.927846	-0.025777	2.873680
128.630419	2720.344361	5.932851	-0.025854	2.877626
128.926127	2728.391219	5.937856	-0.025915	2.881591
129.208219	2736.398568	5.942861	-0.025973	2.885531
129.625910	2744.429382	5.947866	-0.026056	2.889483
129.890780	2752.533157	5.952870	-0.026111	2.893458
130.018994	2760.571197	5.957875	-0.026140	2.897388
130.463329	2768.598052	5.962880	-0.026229	2.901324
130.530900	2776.641743	5.967885	-0.026247	2.905242
130.524903	2784.701241	5.972890	-0.026251	2.909159
130.973697	2792.816787	5.977894	-0.026340	2.913122
131.061887	2800.841476	5.982899	-0.026362	2.917016
131.332066	2808.846648	5.987904	-0.026418	2.920906
131.509667	2816.823668	5.992909	-0.026456	2.924771
131.637056	2824.850485	5.997914	-0.026486	2.928653
131.861415	2832.922802	6.002918	-0.026533	2.932557
132.160165	2840.938855	6.007923	-0.026594	2.936432
132.355889	2848.970372	6.012928	-0.026636	2.940305
132.648220	2856.982585	6.017933	-0.026696	2.944167
132.799994	2865.022019	6.022938	-0.026730	2.948031
133.062828	2873.090079	6.027942	-0.026784	2.951909
133.154917	2881.142267	6.032947	-0.026807	2.955765
133.351150	2889.174183	6.037952	-0.026849	2.959612
133.799210	2897.154861	6.042957	-0.026938	2.963442
133.785883	2905.227788	6.047962	-0.026941	2.967288
134.033067	2913.283264	6.052966	-0.026993	2.971134
134.313402	2921.317500	6.057971	-0.027050	2.974966
134.503573	2929.344894	6.062976	-0.027091	2.978785
134.873769	2937.356256	6.067981	-0.027166	2.982601
135.227370	2945.385787	6.072986	-0.027237	2.986420
135.323715	2953.468314	6.077990	-0.027260	2.990246
135.548366	2961.517213	6.082995	-0.027308	2.994058
136.046852	2969.518366	6.088000	-0.027406	2.997856
136.288712	2977.545766	6.093005	-0.027457	3.001649
136.607203	2985.561425	6.098010	-0.027521	3.005435
136.903413	2993.592372	6.103014	-0.027582	3.009222
137.036738	3001.659367	6.108019	-0.027612	3.013013
137.257534	3009.728095	6.113024	-0.027659	3.016805
137.480164	3017.759511	6.118029	-0.027706	3.020574
137.598959	3025.756454	6.123034	-0.027734	3.024318
137.856254	3033.812509	6.128038	-0.027787	3.028091
137.980870	3041.867771	6.133043	-0.027816	3.031853
138.191141	3049.930922	6.138048	-0.027861	3.035618
138.367269	3057.909669	6.143053	-0.027899	3.039337
138.529439	3065.954208	6.148058	-0.027935	3.043082
138.799125	3073.980808	6.153062	-0.027990	3.046818
139.046579	3081.996778	6.158067	-0.028042	3.050544
139.300390	3090.071307	6.163072	-0.028095	3.054293
139.550513	3098.084634	6.168077	-0.028147	3.058009
139.737074	3106.117744	6.173082	-0.028187	3.061726
140.096263	3114.137637	6.178086	-0.028259	3.065441
140.251925	3122.166530	6.183091	-0.028294	3.069146
140.561866	3130.297474	6.188096	-0.028357	3.072901
140.763909	3138.346148	6.193101	-0.028400	3.076608
140.919334	3146.337888	6.198106	-0.028435	3.080282
141.390024	3154.327757	6.203110	-0.028528	3.083966
141.306444	3162.348686	6.208115	-0.028518	3.087633
141.482829	3170.430081	6.213120	-0.028556	3.091336
141.649575	3178.451091	6.218125	-0.028593	3.095007
141.801256	3186.483230	6.223130	-0.028627	3.098678
142.237997	3194.475796	6.228134	-0.028713	3.102339
142.347854	3202.496361	6.233139	-0.028739	3.105993
142.648145	3210.562384	6.238144	-0.028801	3.109673
142.790006	3218.634663	6.243149	-0.028833	3.113344
143.096042	3226.642325	6.248154	-0.028895	3.116988
143.273228	3234.674398	6.253158	-0.028934	3.120634
143.730366	3242.636396	6.258163	-0.029024	3.124256
143.928573	3250.695734	6.263168	-0.029067	3.127906
144.045004	3258.761598	6.268173	-0.029094	3.131552
144.099155	3266.840991	6.273178	-0.029110	3.135196
144.323380	3274.843005	6.278182	-0.029157	3.138809
144.499209	3282.854944	6.283187	-0.029195	3.142420
144.969986	3290.883444	6.288192	-0.029288	3.146047
145.087877	3298.914205	6.293197	-0.029316	3.149655
145.168992	3307.006625	6.298202	-0.029336	3.153285
145.506169	3315.009497	6.303206	-0.029405	3.156883
145.704880	3323.010687	6.308211	-0.029447	3.160469
146.134196	3331.009881	6.313216	-0.029533	3.164060
146.023951	3339.070648	6.318221	-0.029518	3.167651
146.390871	3347.093689	6.323226	-0.029591	3.171242
146.656538	3355.156838	6.328230	-0.029646	3.174843
146.747446	3363.172329	6.333235	-0.029669	3.178410
147.207382	3371.202924	6.338240	-0.029760	3.181996
147.289537	3379.252982	6.343245	-0.029781	3.185570
147.418011	3387.268923	6.348250	-0.029810	3.189128
147.836624	3395.328290	6.353254	-0.029894	3.192712
148.041640	3403.354399	6.358259	-0.029937	3.196269
148.101524	3411.363746	6.363264	-0.029954	3.199809
148.244513	3419.394648	6.368269	-0.029986	3.203357
148.520726	3427.416244	6.373274	-0.030043	3.206903
148.740423	3435.465690	6.378278	-0.030089	3.210455
148.874150	3443.500301	6.383283	-0.030120	3.213993
149.248869	3451.521866	6.388288	-0.030195	3.217531
149.499340	3459.555579	6.393293	-0.030247	3.221065
149.546447	3467.558854	6.398298	-0.030262	3.224574
149.995107	3475.603966	6.403302	-0.030351	3.228114
150.276567	3483.660887	6.408307	-0.030409	3.231648
150.545958	3491.752932	6.413312	-0.030464	3.235193
150.546319	3499.747251	6.418317	-0.030470	3.238681
150.793721	3507.740898	6.423322	-0.030521	3.242174
151.155247	3515.744211	6.428326	-0.030594	3.245673
151.052419	3523.766914	6.433331	-0.030581	3.249157
151.457659	3531.829737	6.438336	-0.030662	3.252676
151.617858	3539.875804	6.443341	-0.030697	3.256173
151.832636	3547.856410	6.448346	-0.030742	3.259641
152.268702	3555.891733	6.453350	-0.030829	3.263137
152.391630	3563.920458	6.458355	-0.030858	3.266614
152.494052	3571.977029	6.463360	-0.030882	3.270099
152.508521	3580.035057	6.468365	-0.030890	3.273577
152.969913	3588.042967	6.473370	-0.030982	3.277048
153.481335	3596.068122	6.478374	-0.031082	3.280524
153.465350	3604.073493	6.483379	-0.031085	3.283967
153.941527	3612.123542	6.488384	-0.031179	3.287445
154.093194	3620.163547	6.493389	-0.031213	3.290902
154.144698	3628.213074	6.498394	-0.031228	3.294356
154.418358	3636.230749	6.503398	-0.031285	3.297801
154.771485	3644.219911	6.508403	-0.031356	3.301234
155.333690	3652.234710	6.513408	-0.031466	3.304681
155.247206	3660.280819	6.518413	-0.031455	3.308114
155.390013	3668.348559	6.523418	-0.031488	3.311561
155.826491	3676.359892	6.528422	-0.031574	3.314991
155.829681	3684.376985	6.533427	-0.031580	3.318404
156.057066	3692.381814	6.538432	-0.031628	3.321817
156.134523	3700.415552	6.543437	-0.031648	3.325233
156.384190	3708.420377	6.548442	-0.031700	3.328639
156.494654	3716.495840	6.553446	-0.031726	3.332067
156.592361	3724.526216	6.558451	-0.031750	3.335471
156.917951	3732.530926	6.563456	-0.031816	3.338870
157.065661	3740.560191	6.568461	-0.031849	3.342269
157.294701	3748.567704	6.573466	-0.031897	3.345658
157.734658	3756.584417	6.578470	-0.031985	3.349056
157.897150	3764.645359	6.583475	-0.032020	3.352458
157.901066	3772.743107	6.588480	-0.032027	3.355867
158.195728	3780.733426	6.593485	-0.032087	3.359237
158.500958	3788.735471	6.598490	-0.032149	3.362609
158.444175	3796.806518	6.603494	-0.032144	3.365994
158.650804	3804.775956	6.608499	-0.032188	3.369343
158.760806	3812.875046	6.613504	-0.032214	3.372739
159.075750	3820.901442	6.618509	-0.032279	3.376108
159.297101	3828.886420	6.623514	-0.032325	3.379453
159.505116	3836.920202	6.628518	-0.032369	3.382815
159.550922	3844.932369	6.633523	-0.032383	3.386158
159.796607	3852.985839	6.638528	-0.032435	3.389523
160.072296	3861.063669	6.643533	-0.032492	3.392895
160.329728	3869.106893	6.648538	-0.032545	3.396249
160.668424	3877.068686	6.653542	-0.032614	3.399569
160.775992	3885.039690	6.658547	-0.032639	3.402881
161.165609	3893.086142	6.663552	-0.032717	3.406231
161.199406	3901.127336	6.668557	-0.032729	3.409563
161.367537	3909.138095	6.673562	-0.032766	3.412884
161.683935	3917.194327	6.678566	-0.032830	3.416226
161.447880	3925.196864	6.683571	-0.032792	3.419523
162.060522	3933.187774	6.688576	-0.032911	3.422841
162.327686	3941.231061	6.693581	-0.032967	3.426165
162.247912	3949.302415	6.698586	-0.032957	3.429487
162.484320	3957.330629	6.703590	-0.033007	3.432797
162.731278	3965.342292	6.708595	-0.033058	3.436099
163.083900	3973.337200	6.713600	-0.033129	3.439393
163.137851	3981.372595	6.718605	-0.033145	3.442691
163.447765	3989.369063	6.723610	-0.033208	3.445979
163.659591	3997.429315	6.728614	-0.033253	3.449286
163.727285	4005.501402	6.733619	-0.033271	3.452590
164.071647	4013.536062	6.738624	-0.033341	3.455885
164.213407	4021.551214	6.743629	-0.033373	3.459161
164.479280	4029.540358	6.748634	-0.033428	3.462429
164.796785	4037.575981	6.753638	-0.033493	3.465713
164.923803	4045.607711	6.758643	-0.033522	3.468987
165.257869	4053.668265	6.763648	-0.033589	3.472276
165.493629	4061.694454	6.768653	-0.033639	3.475545
165.461203	4069.692594	6.773658	-0.033638	3.478790
165.962517	4077.705362	6.778662	-0.033737	3.482056
166.012713	4085.702048	6.783667	-0.033752	3.485298
166.902299	4093.733656	6.788672	-0.033923	3.488577
167.058178	4101.756573	6.793677	-0.033958	3.491826
167.461822	4109.777732	6.798682	-0.034038	3.495080
167.673345	4117.838561	6.803686	-0.034083	3.498340
167.604740	4125.832750	6.808691	-0.034076	3.501562
168.018071	4133.848066	6.813696	-0.034158	3.504804
168.152238	4141.887945	6.818701	-0.034189	3.508044
168.368715	4149.936742	6.823706	-0.034235	3.511288
168.782483	4157.973237	6.828710	-0.034317	3.514529
168.876087	4165.974233	6.833715	-0.034340	3.517744
169.134512	4174.018266	6.838720	-0.034394	3.520977
169.298300	4182.012342	6.843725	-0.034430	3.524185
169.451124	4190.047394	6.848730	-0.034464	3.527406
169.814078	4198.054371	6.853734	-0.034537	3.530619
169.840340	4206.107631	6.858739	-0.034547	3.533838
170.100785	4214.158369	6.863744	-0.034601	3.537060
170.107529	4222.181669	6.868749	-0.034608	3.540260
170.150614	4230.185205	6.873754	-0.034622	3.543450
170.465843	4238.227346	6.878758	-0.034686	3.546661
170.648984	4246.264823	6.883763	-0.034725	3.549863
170.886760	4254.395965	6.888768	-0.034775	3.553101
170.932813	4262.389992	6.893773	-0.034789	3.556276
171.101278	4270.338792	6.898778	-0.034826	3.559434
171.312109	4278.357803	6.903782	-0.034871	3.562618
171.350867	4286.388912	6.908787	-0.034884	3.565799
171.685504	4294.406211	6.913792	-0.034951	3.568981
171.844768	4302.423951	6.918797	-0.034987	3.572154
171.987478	4310.459607	6.923802	-0.035019	3.575332
172.286221	4318.462579	6.928806	-0.035080	3.578498
172.336626	4326.489298	6.933811	-0.035095	3.581663
172.519493	4334.504002	6.938816	-0.035134	3.584825
172.483610	4342.524267	6.943821	-0.035133	3.587979
172.596679	4350.585305	6.948826	-0.035160	3.591152
172.973530	4358.596339	6.953830	-0.035235	3.594309
173.063553	4366.591447	6.958835	-0.035258	3.597449
173.412690	4374.605276	6.963840	-0.035328	3.600601
173.820293	4382.576664	6.968845	-0.035410	3.603735
173.607009	4390.652939	6.973850	-0.035375	3.606890
173.849959	4398.686969	6.978854	-0.035426	3.610039
174.113723	4406.721058	6.983859	-0.035481	3.613185
174.353233	4414.779995	6.988864	-0.035531	3.616338
174.449748	4422.735247	6.993869	-0.035554	3.619443
174.803186	4430.777889	6.998874	-0.035626	3.622587
175.047053	4438.785637	7.003878	-0.035677	3.625712
175.049153	4446.826157	7.008883	-0.035682	3.628840
175.186689	4454.902747	7.013888	-0.035714	3.631982
175.381258	4462.942219	7.018893	-0.035755	3.635110
175.509623	4470.925684	7.023898	-0.035785	3.638211
175.495069	4478.993591	7.028902	-0.035788	3.641338
175.761093	4486.936185	7.033907	-0.035843	3.644422
176.383796	4494.971660	7.038912	-0.035964	3.647548
176.383489	4503.011015	7.043917	-0.035969	3.650657
176.651800	4511.055832	7.048922	-0.036025	3.653772
177.025223	4519.088335	7.053926	-0.036100	3.656882
177.040904	4527.050956	7.058931	-0.036108	3.659954
177.309691	4535.124691	7.063936	-0.036164	3.663072
177.471601	4543.157500	7.068941	-0.036200	3.666169
177.491007	4551.159700	7.073946	-0.036209	3.669248
177.577580	4559.223441	7.078950	-0.036230	3.672350
177.720620	4567.235770	7.083955	-0.036263	3.675430
178.265616	4575.208486	7.088960	-0.036369	3.678504
178.217092	4583.243976	7.093965	-0.036366	3.681583
178.439774	4591.226572	7.098970	-0.036413	3.684647
178.815132	4599.275163	7.103974	-0.036488	3.687737
179.057885	4607.275738	7.108979	-0.036539	3.690803
179.024379	4615.376480	7.113984	-0.036538	3.693897
179.203341	4623.372701	7.118989	-0.036577	3.696955
179.524248	4631.372065	7.123994	-0.036642	3.700014
179.817381	4639.368541	7.128998	-0.036702	3.703070
180.026850	4647.410009	7.134003	-0.036747	3.706137
180.379749	4655.419383	7.139008	-0.036818	3.709194
180.192410	4663.530454	7.144013	-0.036789	3.712273
180.557986	4671.582094	7.149018	-0.036862	3.715341
180.667716	4679.556626	7.154022	-0.036888	3.718370
180.833613	4687.535762	7.159027	-0.036925	3.721400
180.952410	4695.517076	7.164032	-0.036952	3.724428
181.067459	4703.551375	7.169037	-0.036979	3.727473
181.318379	4711.561379	7.174042	-0.037031	3.730509
181.552368	4719.644373	7.179046	-0.037081	3.733570
181.514640	4727.667753	7.184051	-0.037079	3.736600
181.857856	4735.633101	7.189056	-0.037148	3.739614
182.200791	4743.678767	7.194061	-0.037218	3.742656
182.244152	4751.674448	7.199066	-0.037231	3.745670
182.486475	4759.723088	7.204070	-0.037282	3.748706
182.427690	4767.789616	7.209075	-0.037277	3.751739
182.723789	4775.825700	7.214080	-0.037337	3.754766
183.005182	4783.819418	7.219085	-0.037395	3.757775
183.094086	4791.857331	7.224090	-0.037417	3.760793
183.244850	4799.837144	7.229094	-0.037451	3.763789
183.253230	4807.864613	7.234099	-0.037458	3.766796
183.923330	4815.899021	7.239104	-0.037588	3.769820
183.860586	4823.958862	7.244109	-0.037582	3.772833
183.873260	4831.987129	7.249114	-0.037590	3.775834
184.132097	4839.984341	7.254118	-0.037644	3.778826
184.370205	4847.990936	7.259123	-0.037693	3.781819
184.498986	4855.997984	7.264128	-0.037723	3.784808
184.642218	4864.034032	7.269133	-0.037755	3.787805
184.869322	4872.063124	7.274138	-0.037803	3.790799
184.976504	4880.136866	7.279142	-0.037828	3.793804
185.106122	4888.151872	7.284147	-0.037858	3.796786
185.377253	4896.098447	7.289152	-0.037914	3.799743
185.524837	4904.115000	7.294157	-0.037947	3.802721
185.535140	4912.146807	7.299162	-0.037954	3.805700
185.804902	4920.155415	7.304166	-0.038010	3.808673
186.091738	4928.192188	7.309171	-0.038069	3.811654
186.191475	4936.233591	7.314176	-0.038093	3.814631
186.502211	4944.260662	7.319181	-0.038156	3.817605
187.008038	4952.204234	7.324186	-0.038256	3.820550
186.909195	4960.289640	7.329190	-0.038243	3.823531
186.755794	4968.311612	7.334195	-0.038220	3.826486
187.239121	4976.313531	7.339200	-0.038316	3.829445
187.354673	4984.353817	7.344205	-0.038343	3.832408
187.385566	4992.341516	7.349210	-0.038354	3.835347
187.796444	5000.398841	7.354214	-0.038436	3.838318
188.007675	5008.359908	7.359219	-0.038481	3.841247
188.188033	5016.379936	7.364224	-0.038520	3.844194
188.234075	5024.433307	7.369229	-0.038534	3.847149
188.272643	5032.466042	7.374234	-0.038547	3.850093
188.735676	5040.491604	7.379238	-0.038638	3.853042
188.644182	5048.543124	7.384243	-0.038627	3.855986
188.633841	5056.563832	7.389248	-0.038630	3.858919
189.064302	5064.539057	7.394253	-0.038716	3.861841
189.280667	5072.545077	7.399258	-0.038762	3.864768
189.458149	5080.623600	7.404262	-0.038800	3.867719
189.595399	5088.636024	7.409267	-0.038832	3.870642
189.846046	5096.907379	7.414272	-0.038884	3.873660
189.929169	5104.871692	7.419277	-0.038905	3.876560
190.049357	5112.724946	7.424282	-0.038933	3.879419
190.450692	5120.776951	7.429286	-0.039013	3.882353
190.430837	5128.731298	7.434291	-0.039015	3.885241
190.882049	5136.739652	7.439296	-0.039104	3.888156
190.888414	5144.777804	7.444301	-0.039111	3.891071
191.126039	5152.817535	7.449306	-0.039161	3.893988
191.213953	5160.857482	7.454310	-0.039182	3.896901
191.328112	5168.794202	7.459315	-0.039209	3.899774
191.671972	5176.867381	7.464320	-0.039279	3.902699
191.902731	5184.862741	7.469325	-0.039327	3.905592
192.002244	5192.870941	7.474330	-0.039351	3.908484
192.263646	5200.947762	7.479334	-0.039405	3.911402
192.224320	5208.944829	7.484339	-0.039404	3.914284
192.758825	5216.980794	7.489344	-0.039509	3.917188
192.735445	5224.954259	7.494349	-0.039510	3.920057
192.688914	5232.970348	7.499354	-0.039507	3.922939
193.113195	5241.019731	7.504358	-0.039591	3.925839
193.129639	5249.003656	7.509363	-0.039600	3.928707
193.354914	5257.046462	7.514368	-0.039647	3.931597
193.479766	5265.094225	7.519373	-0.039676	3.934485
193.587487	5273.111335	7.524378	-0.039701	3.937359
193.948202	5281.106949	7.529382	-0.039774	3.940228
193.966362	5289.083615	7.534387	-0.039783	3.943082
194.267592	5297.124620	7.539392	-0.039845	3.945962
194.458125	5305.142106	7.544397	-0.039886	3.948830
194.529091	5313.244850	7.549402	-0.039904	3.951724
194.788333	5321.272601	7.554406	-0.039958	3.954592
194.873774	5329.210474	7.559411	-0.039980	3.957423
195.052382	5337.229356	7.564416	-0.040018	3.960282
195.247758	5345.195401	7.569421	-0.040060	3.963121
195.558009	5353.230226	7.574426	-0.040123	3.965984
195.758283	5361.263948	7.579430	-0.040166	3.968843
195.727027	5369.320727	7.584435	-0.040166	3.971704
196.024922	5377.334275	7.589440	-0.040227	3.974553
196.256425	5385.360363	7.594445	-0.040276	3.977404
196.486788	5393.364168	7.599450	-0.040324	3.980244
196.671574	5401.410321	7.604454	-0.040364	3.983097
196.850178	5409.422904	7.609459	-0.040403	3.985935
196.818340	5417.443981	7.614464	-0.040402	3.988771
197.009859	5425.494024	7.619469	-0.040443	3.991619
197.037775	5433.508791	7.624474	-0.040454	3.994450
197.642769	5441.536452	7.629478	-0.040572	3.997292
197.607174	5449.489494	7.634483	-0.040571	4.000096
197.789657	5457.531263	7.639488	-0.040611	4.002933
198.071306	5465.534423	7.644493	-0.040668	4.005756
198.149514	5473.585357	7.649498	-0.040689	4.008590
198.212533	5481.687122	7.654502	-0.040706	4.011439
198.652112	5489.650766	7.659507	-0.040793	4.014245
198.922064	5497.687307	7.664512	-0.040849	4.017071
199.020279	5505.673144	7.669517	-0.040873	4.019874
199.175995	5513.712841	7.674522	-0.040907	4.022695
199.284131	5521.761236	7.679526	-0.040933	4.025517
199.335591	5529.782127	7.684531	-0.040948	4.028326
199.577418	5537.800368	7.689536	-0.040999	4.031136
199.775317	5545.891421	7.694541	-0.041041	4.033967
199.705554	5553.868386	7.699546	-0.041033	4.036754
200.135162	5561.836575	7.704550	-0.041119	4.039542
200.052628	5569.861866	7.709555	-0.041109	4.042341
200.395288	5577.851328	7.714560	-0.041178	4.045132
200.748498	5585.872904	7.719565	-0.041250	4.047932
200.911424	5593.866046	7.724570	-0.041285	4.050717
201.190004	5601.952370	7.729574	-0.041343	4.053535
201.337337	5609.954710	7.734579	-0.041376	4.056319
201.486203	5617.923005	7.739584	-0.041409	4.059090
201.679441	5625.953446	7.744589	-0.041450	4.061881
202.097186	5633.912754	7.749594	-0.041534	4.064649
202.158558	5641.976028	7.754598	-0.041551	4.067446
202.286062	5649.977295	7.759603	-0.041580	4.070220
202.409811	5658.048273	7.764608	-0.041608	4.073016
202.477093	5666.084715	7.769613	-0.041627	4.075798
202.621722	5674.028741	7.774618	-0.041659	4.078547
202.898637	5682.096728	7.779622	-0.041716	4.081339
202.868726	5690.042381	7.784627	-0.041716	4.084082
202.825624	5698.126936	7.789632	-0.041713	4.086871
203.178331	5706.119901	7.794637	-0.041785	4.089632
203.409670	5714.133150	7.799642	-0.041833	4.092397
203.496824	5722.202889	7.804646	-0.041855	4.095177
203.493470	5730.180936	7.809651	-0.041860	4.097922
203.875594	5738.197584	7.814656	-0.041936	4.100684
204.117441	5746.202475	7.819661	-0.041987	4.103439
204.141643	5754.189344	7.824666	-0.041997	4.106182
204.650710	5762.285069	7.829670	-0.042097	4.108967
204.548274	5770.330421	7.834675	-0.042084	4.111725
204.676355	5778.368820	7.839680	-0.042113	4.114482
204.879155	5786.377046	7.844685	-0.042156	4.117227
205.131704	5794.325899	7.849690	-0.042209	4.119951
205.302244	5802.381772	7.854694	-0.042246	4.122709
205.352026	5810.358031	7.859699	-0.042261	4.125436
205.752354	5818.390741	7.864704	-0.042341	4.128185
205.971368	5826.452060	7.869709	-0.042387	4.130939
206.132923	5834.440378	7.874714	-0.042423	4.133666
206.441345	5842.503869	7.879718	-0.042486	4.136419
206.476298	5850.502925	7.884723	-0.042498	4.139145
206.814167	5858.528571	7.889728	-0.042566	4.141881
206.998153	5866.522909	7.894733	-0.042606	4.144603
206.958088	5874.555296	7.899738	-0.042604	4.147334
207.039470	5882.597897	7.904742	-0.042625	4.150067
207.106685	5890.623342	7.909747	-0.042643	4.152793
207.522487	5898.643835	7.914752	-0.042726	4.155520
207.577499	5906.645390	7.919757	-0.042741	4.158234
207.699224	5914.643463	7.924762	-0.042769	4.160945
207.899847	5922.645039	7.929766	-0.042812	4.163657
208.055507	5930.678365	7.934771	-0.042847	4.166378
207.971295	5938.696483	7.939776	-0.042837	4.169089
208.072271	5946.732060	7.944781	-0.042861	4.171806
208.407052	5954.749408	7.949786	-0.042929	4.174518
208.489921	5962.778618	7.954790	-0.042950	4.177229
208.401685	5970.756697	7.959795	-0.042939	4.179919
208.746350	5978.786844	7.964800	-0.043009	4.182630
208.887073	5986.753904	7.969805	-0.043040	4.185315
208.988917	5994.810893	7.974810	-0.043065	4.188029
209.368853	6002.846570	7.979814	-0.043141	4.190737
209.561049	6010.950274	7.984819	-0.043182	4.193463
209.686524	6018.939704	7.989824	-0.043211	4.196149
209.969267	6026.907020	7.994829	-0.043269	4.198828
210.138336	6034.934303	7.999834	-0.043306	4.201523
210.309909	6042.881996	8.004838	-0.043344	4.204190
210.175269	6050.921656	8.009843	-0.043324	4.206883
210.532741	6058.930737	8.014848	-0.043396	4.209570
210.663113	6067.003362	8.019853	-0.043426	4.212273
210.897235	6074.954835	8.024858	-0.043475	4.214935
211.217420	6083.048038	8.029862	-0.043540	4.217644
211.403362	6090.977670	8.034867	-0.043580	4.220295
211.576211	6099.025014	8.039872	-0.043618	4.222983
211.668726	6107.067779	8.044877	-0.043641	4.225667
212.036032	6115.051410	8.049882	-0.043715	4.228333
212.320492	6123.112017	8.054886	-0.043773	4.231021
212.149207	6131.134854	8.059891	-0.043747	4.233691
212.602510	6139.182195	8.064896	-0.043837	4.236374
212.826488	6147.120272	8.069901	-0.043884	4.239016
212.803551	6155.176611	8.074906	-0.043885	4.241693
213.065377	6163.147244	8.079910	-0.043939	4.244343
213.332354	6171.217850	8.084915	-0.043995	4.247025
213.481807	6179.183041	8.089920	-0.044028	4.249669
213.692760	6187.264598	8.094925	-0.044073	4.252350
213.856326	6195.232000	8.099930	-0.044109	4.254991
213.869919	6203.300956	8.104934	-0.044117	4.257663
213.800230	6211.286650	8.109939	-0.044109	4.260305
214.038078	6219.311496	8.114944	-0.044159	4.262960
214.242149	6227.300775	8.119949	-0.044202	4.265603
214.427794	6235.359885	8.124954	-0.044243	4.268266
214.515392	6243.407773	8.129958	-0.044264	4.270923
214.722614	6251.462323	8.134963	-0.044308	4.273582
215.007687	6259.460277	8.139968	-0.044367	4.276221
215.172819	6267.421832	8.144973	-0.044403	4.278845
215.377053	6275.439519	8.149978	-0.044447	4.281487
215.464757	6283.427239	8.154982	-0.044469	4.284116
215.556525	6291.473941	8.159987	-0.044491	4.286763
215.847032	6299.460828	8.164992	-0.044551	4.289390
215.942404	6307.563121	8.169997	-0.044574	4.292052
215.935862	6315.546452	8.175002	-0.044578	4.294672
216.073125	6323.611127	8.180006	-0.044609	4.297318
216.178692	6331.562526	8.185011	-0.044635	4.299926
216.418386	6339.621388	8.190016	-0.044685	4.302568
216.591295	6347.599149	8.195021	-0.044722	4.305181
216.717967	6355.576246	8.200026	-0.044751	4.307793
216.965942	6363.648989	8.205030	-0.044803	4.310435
216.871263	6371.693664	8.210035	-0.044791	4.313063
217.000820	6379.737094	8.215040	-0.044821	4.315691
217.231372	6387.705685	8.220045	-0.044869	4.318294
217.183275	6395.682623	8.225050	-0.044866	4.320896
217.401493	6403.761832	8.230054	-0.044912	4.323531
217.569674	6411.720660	8.235059	-0.044949	4.326126
217.907538	6419.725673	8.240064	-0.045017	4.328735
217.953587	6427.825531	8.245069	-0.045031	4.331371
218.019597	6435.806048	8.250074	-0.045049	4.333967
218.321643	6443.857415	8.255078	-0.045111	4.336586
218.187099	6451.809625	8.260083	-0.045091	4.339168
218.226116	6459.830205	8.265088	-0.045104	4.341772
218.462756	6467.803366	8.270093	-0.045153	4.344361
218.489304	6475.860859	8.275098	-0.045164	4.346974
218.626622	6483.902636	8.280102	-0.045195	4.349580
218.784592	6491.942132	8.285107	-0.045230	4.352185
219.043711	6500.004744	8.290112	-0.045284	4.354796
219.079402	6508.002418	8.295117	-0.045296	4.357384
219.025071	6515.934190	8.300122	-0.045291	4.359947
219.446884	6523.981176	8.305126	-0.045375	4.362550
219.444678	6531.975575	8.310131	-0.045380	4.365131
219.564319	6539.992704	8.315136	-0.045408	4.367719
219.810391	6547.995786	8.320141	-0.045459	4.370301
219.778849	6556.010853	8.325146	-0.045459	4.372885
219.977021	6564.061293	8.330150	-0.045501	4.375479
220.049384	6572.030633	8.335155	-0.045520	4.378045
220.395164	6580.049219	8.340160	-0.045590	4.380627
220.375933	6588.102554	8.345165	-0.045592	4.383216
220.349676	6596.112187	8.350170	-0.045593	4.385790
220.698719	6604.149092	8.355174	-0.045663	4.388373
220.532604	6612.161896	8.360179	-0.045638	4.390944
220.657760	6620.197694	8.365184	-0.045667	4.393523
220.809058	6628.227110	8.370189	-0.045700	4.396098
221.000246	6636.162190	8.375194	-0.045741	4.398641
221.245010	6644.217110	8.380198	-0.045793	4.401222
221.278490	6652.195438	8.385203	-0.045804	4.403775
221.492365	6660.265318	8.390208	-0.045850	4.406357
221.600566	6668.280171	8.395213	-0.045875	4.408920
221.851165	6676.299438	8.400218	-0.045927	4.411483
222.190876	6684.368054	8.405222	-0.045996	4.414061
222.080404	6692.351595	8.410227	-0.045981	4.416608
222.195869	6700.334304	8.415232	-0.046008	4.419154
222.424490	6708.405212	8.420237	-0.046056	4.421728
222.482393	6716.366791	8.425242	-0.046073	4.424264
222.457614	6724.433260	8.430246	-0.046073	4.426832
222.778736	6732.438549	8.435251	-0.046139	4.429380
223.117041	6740.489588	8.440256	-0.046207	4.431942
223.183029	6748.551228	8.445261	-0.046225	4.434504
223.205329	6756.490350	8.450266	-0.046235	4.437026
223.483578	6764.514123	8.455270	-0.046292	4.439574
223.626790	6772.510979	8.460275	-0.046324	4.442112
223.593772	6780.491179	8.465280	-0.046323	4.444642
223.678737	6788.565041	8.470285	-0.046345	4.447200
223.901914	6796.522493	8.475290	-0.046392	4.449721
223.952557	6804.597255	8.480294	-0.046407	4.452277
224.116590	6812.625904	8.485299	-0.046443	4.454818
224.270556	6820.626736	8.490304	-0.046477	4.457348
224.553191	6828.609866	8.495309	-0.046535	4.459871
224.571904	6836.630457	8.500314	-0.046544	4.462404
224.860891	6844.617812	8.505318	-0.046603	4.464926
224.987578	6852.687916	8.510323	-0.046633	4.467472
224.959794	6860.677263	8.515328	-0.046633	4.469991
225.244193	6868.710247	8.520333	-0.046691	4.472523
225.527587	6876.716179	8.525338	-0.046750	4.475045
225.784671	6884.791532	8.530342	-0.046803	4.477587
225.864626	6892.717576	8.535347	-0.046823	4.480080
226.253118	6900.741234	8.540352	-0.046901	4.482604
226.489856	6908.746271	8.545357	-0.046951	4.485119
226.315075	6916.794829	8.550362	-0.046924	4.487646
226.711776	6924.808425	8.555366	-0.047003	4.490162
226.920441	6932.847406	8.560371	-0.047047	4.492684
227.018484	6940.845211	8.565376	-0.047071	4.495191
227.070233	6948.865898	8.570381	-0.047086	4.497704
227.088257	6956.851509	8.575386	-0.047095	4.500205
227.448305	6964.910408	8.580391	-0.047168	4.502727
227.500714	6972.884771	8.585395	-0.047183	4.505222
227.585587	6980.880291	8.590400	-0.047204	4.507721
227.744310	6988.966650	8.595405	-0.047239	4.510248
227.807188	6997.011376	8.600410	-0.047257	4.512760
227.910828	7005.049290	8.605415	-0.047281	4.515268
227.895563	7013.009526	8.610419	-0.047284	4.517751
228.083056	7020.967619	8.615424	-0.047324	4.520232
228.371842	7029.034683	8.620429	-0.047384	4.522746
228.679492	7036.981855	8.625434	-0.047447	4.525221
228.689558	7045.032897	8.630439	-0.047454	4.527726
228.674896	7053.045400	8.635443	-0.047457	4.530218
229.033997	7061.082997	8.640448	-0.047529	4.532717
229.196421	7069.122398	8.645453	-0.047565	4.535215
229.014369	7077.077888	8.650458	-0.047536	4.537685
229.369663	7085.102902	8.655463	-0.047608	4.540176
229.502020	7093.124684	8.660467	-0.047638	4.542664
229.699059	7101.139485	8.665472	-0.047680	4.545149
229.813802	7109.133996	8.670477	-0.047707	4.547626
229.994968	7117.140647	8.675482	-0.047746	4.550106
230.188798	7125.241491	8.680487	-0.047788	4.552613
230.166051	7133.228774	8.685491	-0.047789	4.555083
230.121741	7141.231602	8.690496	-0.047787	4.557557
230.323836	7149.253869	8.695501	-0.047830	4.560036
230.338665	7157.254062	8.700506	-0.047838	4.562507
230.863705	7165.254560	8.705511	-0.047941	4.564976
230.777070	7173.321641	8.710515	-0.047931	4.567465
230.840791	7181.297340	8.715520	-0.047948	4.569924
231.208795	7189.373637	8.720525	-0.048022	4.572412
231.213323	7197.360321	8.725530	-0.048028	4.574872
231.427158	7205.426784	8.730535	-0.048074	4.577355
231.311714	7213.378849	8.735539	-0.048058	4.579801
231.318178	7221.410990	8.740544	-0.048064	4.582270
231.571394	7229.401149	8.745549	-0.048117	4.584726
231.682448	7237.409231	8.750554	-0.048143	4.587185
231.766490	7245.455291	8.755559	-0.048164	4.589655
231.808579	7253.526161	8.760563	-0.048178	4.592131
232.055718	7261.523674	8.765568	-0.048229	4.594584
232.209644	7269.580726	8.770573	-0.048263	4.597053
232.094063	7277.467146	8.775578	-0.048247	4.599468
232.678538	7285.515060	8.780583	-0.048362	4.601932
232.769253	7293.510785	8.785587	-0.048384	4.604379
232.881910	7301.554705	8.790592	-0.048411	4.606838
233.095557	7309.615191	8.795597	-0.048456	4.609302
233.281913	7317.575812	8.800602	-0.048496	4.611734
233.138387	7325.631773	8.805607	-0.048475	4.614193
233.452227	7333.636778	8.810611	-0.048539	4.616636
233.628150	7341.614366	8.815616	-0.048577	4.619069
233.737095	7349.693530	8.820621	-0.048603	4.621532
233.761895	7357.636563	8.825626	-0.048613	4.623951
233.943181	7365.698782	8.830631	-0.048652	4.626406
233.979656	7373.682086	8.835635	-0.048665	4.628836
234.061299	7381.732292	8.840640	-0.048685	4.631284
234.346496	7389.776830	8.845645	-0.048744	4.633730
234.153075	7397.799237	8.850650	-0.048713	4.636167
234.342228	7405.731913	8.855655	-0.048754	4.638576
234.587463	7413.794430	8.860659	-0.048805	4.641023
234.716740	7421.752956	8.865664	-0.048835	4.643438
234.784995	7429.795867	8.870669	-0.048853	4.645876
234.892852	7437.826657	8.875674	-0.048879	4.648310
235.250131	7445.845919	8.880679	-0.048951	4.650739
235.347438	7453.859445	8.885683	-0.048974	4.653164
235.420066	7461.880215	8.890688	-0.048993	4.655591
235.531706	7469.915667	8.895693	-0.049020	4.658021
235.715032	7477.851273	8.900698	-0.049059	4.660419
235.909791	7485.866553	8.905703	-0.049101	4.662840
236.034928	7493.930276	8.910707	-0.049130	4.665275
236.139665	7501.939198	8.915712	-0.049155	4.667692
236.236227	7509.940895	8.920717	-0.049178	4.670105
236.295060	7518.070911	8.925722	-0.049195	4.672556
236.592724	7526.139004	8.930727	-0.049256	4.674986
236.708781	7534.049778	8.935731	-0.049283	4.677368
236.906354	7542.009674	8.940736	-0.049325	4.679764
237.039082	7550.075114	8.945741	-0.049355	4.682190
237.098168	7557.953284	8.950746	-0.049372	4.684559
237.357515	7566.063159	8.955751	-0.049426	4.686995
237.312183	7574.050784	8.960755	-0.049423	4.689395
237.536258	7582.103441	8.965760	-0.049470	4.691812
237.866748	7590.126678	8.970765	-0.049537	4.694218
237.628011	7598.154606	8.975770	-0.049498	4.696626
237.833368	7606.113511	8.980775	-0.049542	4.699012
238.007221	7614.165972	8.985779	-0.049580	4.701424
238.060944	7622.116454	8.990784	-0.049595	4.703804
238.233934	7630.138646	8.995789	-0.049633	4.706205
238.370693	7638.130285	9.000794	-0.049664	4.708595
238.723116	7646.219627	9.005799	-0.049735	4.711013
238.723297	7654.303168	9.010803	-0.049740	4.713428
238.860670	7662.246638	9.015808	-0.049771	4.715800
239.171893	7670.265703	9.020813	-0.049835	4.718193
239.032927	7678.246416	9.025818	-0.049815	4.720575
239.197411	7686.273544	9.030823	-0.049851	4.722968
239.286914	7694.293672	9.035827	-0.049873	4.725358
239.290746	7702.344380	9.040832	-0.049879	4.727756
239.592181	7710.383068	9.045837	-0.049941	4.730149
239.966666	7718.381522	9.050842	-0.050016	4.732528
240.057938	7726.434959	9.055847	-0.050038	4.734924
240.371324	7734.427483	9.060851	-0.050102	4.737299
240.333085	7742.424814	9.065856	-0.050101	4.739675
240.524208	7750.423247	9.070861	-0.050142	4.742050
240.607281	7758.386770	9.075866	-0.050163	4.744414
240.616870	7766.476669	9.080871	-0.050170	4.746814
240.807209	7774.459955	9.085875	-0.050211	4.749181
240.987865	7782.507253	9.090880	-0.050250	4.751565
241.100321	7790.593746	9.095885	-0.050277	4.753961
241.267201	7798.549994	9.100890	-0.050313	4.756316
241.473573	7806.495944	9.105895	-0.050357	4.758667
241.561896	7814.531085	9.110899	-0.050379	4.761043
241.577834	7822.483859	9.115904	-0.050387	4.763394
241.760843	7830.592675	9.120909	-0.050427	4.765790
241.820703	7838.541300	9.125914	-0.050444	4.768137
242.274256	7846.591915	9.130919	-0.050534	4.770512
242.389699	7854.670980	9.135923	-0.050561	4.772896
242.507540	7862.640866	9.140928	-0.050588	4.775246
242.593315	7870.625961	9.145933	-0.050610	4.777599
242.654431	7878.627425	9.150938	-0.050626	4.779956
242.671850	7886.681060	9.155943	-0.050635	4.782327
242.840139	7894.631499	9.160947	-0.050672	4.784667
243.023066	7902.726228	9.165952	-0.050712	4.787047
243.351542	7910.733661	9.170957	-0.050778	4.789400
243.361771	7918.768231	9.175962	-0.050786	4.791762
243.388110	7926.765549	9.180967	-0.050796	4.794111
243.594294	7934.802430	9.185971	-0.050840	4.796469
243.633412	7942.741893	9.190976	-0.050853	4.798799
243.840006	7950.796367	9.195981	-0.050897	4.801160
243.860216	7958.778540	9.200986	-0.050906	4.803500
244.319039	7966.842827	9.205991	-0.050997	4.805861
244.075303	7974.824529	9.210995	-0.050957	4.808200
244.361022	7982.832314	9.216000	-0.051016	4.810543
244.721751	7990.299934	9.221005	-0.051088	4.812726
244.776413	7994.778736	9.226010	-0.051101	4.814035

244.923583	7997.198336	9.231015	-0.051131	4.814742
245.033777	7998.535956	9.236019	-0.051152	4.815133
244.902850	7999.040008	9.241024	-0.051129	4.815281
244.891097	7999.851437	9.246029	-0.051127	4.815518
245.055590	7999.799681	9.251034	-0.051158	4.815502
245.104595	7999.846425	9.256039	-0.051168	4.815516
245.350478	7999.849392	9.261043	-0.051214	4.815515
245.201371	7999.798928	9.266048	-0.051186	4.815501
245.466849	7999.839591	9.271053	-0.051236	4.815512
245.302747	7999.821988	9.276058	-0.051206	4.815508
245.257571	7999.853314	9.281063	-0.051197	4.815517
245.501919	7999.838101	9.286067	-0.051243	4.815511
245.617816	7999.852831	9.291072	-0.051265	4.815515
245.523772	7999.886563	9.296077	-0.051248	4.815525
245.424810	7999.843324	9.301082	-0.051230	4.815513
245.656838	7999.867424	9.306087	-0.051273	4.815519
245.626441	7999.875496	9.311091	-0.051268	4.815522
245.639467	7999.842627	9.316096	-0.051270	4.815512
245.867536	7999.852780	9.321101	-0.051313	4.815514
245.625610	7999.771967	9.326106	-0.051268	4.815491
245.660567	7999.820618	9.331111	-0.051275	4.815505
245.629373	7999.861783	9.336115	-0.051270	4.815518
245.704848	7999.868379	9.341120	-0.051284	4.815519
245.621276	7999.881991	9.346125	-0.051269	4.815523
245.753901	7999.862820	9.351130	-0.051294	4.815517
245.900599	7999.895140	9.356135	-0.051321	4.815526
245.743562	7999.834934	9.361139	-0.051292	4.815509
245.718064	7999.828135	9.366144	-0.051288	4.815507
245.812087	7999.827557	9.371149	-0.051306	4.815507
245.700689	7999.826832	9.376154	-0.051285	4.815507
246.039099	7999.861212	9.381159	-0.051348	4.815515
246.129918	7999.862718	9.386163	-0.051366	4.815515
246.203204	7999.873550	9.391168	-0.051380	4.815518
246.053219	7999.894622	9.396173	-0.051352	4.815525
245.918828	7999.861483	9.401178	-0.051327	4.815516
246.141781	7999.963397	9.406183	-0.051369	4.815545
246.196789	7999.874611	9.411187	-0.051380	4.815518
246.135876	7999.836264	9.416192	-0.051368	4.815508
246.121444	7999.901197	9.421197	-0.051366	4.815527
245.967806	7999.858133	9.426202	-0.051338	4.815515
246.030059	7999.832475	9.431207	-0.051350	4.815507
246.109319	7999.903209	9.436211	-0.051365	4.815527
246.170494	7999.841223	9.441216	-0.051376	4.815509
246.215230	7999.887899	9.446221	-0.051385	4.815522
246.375190	7999.880922	9.451226	-0.051415	4.815519
246.525563	7999.888740	9.456231	-0.051443	4.815521
246.236364	7999.916084	9.461235	-0.051390	4.815530
246.149609	7999.843140	9.466240	-0.051374	4.815509
246.416472	7999.899849	9.471245	-0.051424	4.815525
246.295995	7999.895771	9.476250	-0.051402	4.815524
246.550702	7999.862574	9.481255	-0.051449	4.815513
246.497817	7999.910861	9.486259	-0.051440	4.815528
246.555112	7999.939588	9.491264	-0.051451	4.815536
246.516608	7999.905877	9.496269	-0.051444	4.815526
246.278295	7999.893469	9.501274	-0.051400	4.815523
246.431489	7999.925896	9.506279	-0.051429	4.815532
246.453803	7999.918809	9.511283	-0.051433	4.815530
246.460145	7999.864471	9.516288	-0.051434	4.815514
246.452791	7999.943404	9.521293	-0.051433	4.815537
246.537723	7999.882873	9.526298	-0.051449	4.815519
246.374549	7999.862080	9.531303	-0.051419	4.815514
246.463729	7999.897734	9.536307	-0.051436	4.815524
246.507338	7999.862160	9.541312	-0.051445	4.815513
246.684125	7999.920603	9.546317	-0.051478	4.815529
246.581424	7999.867689	9.551322	-0.051459	4.815514
246.740865	7999.919443	9.556327	-0.051489	4.815529
246.624606	7999.922909	9.561331	-0.051468	4.815530
246.518447	7999.869939	9.566336	-0.051448	4.815515
246.688980	7999.911193	9.571341	-0.051480	4.815527
246.624108	7999.873848	9.576346	-0.051468	4.815516
246.671878	7999.876788	9.581351	-0.051477	4.815517
246.728631	7999.903370	9.586355	-0.051488	4.815524
246.469034	7999.856439	9.591360	-0.051440	4.815512
246.657144	7999.905456	9.596365	-0.051476	4.815525
246.643835	7999.866817	9.601370	-0.051473	4.815514
246.836826	7999.824068	9.606375	-0.051510	4.815500
246.806040	7999.875921	9.611379	-0.051504	4.815516
246.666345	7999.815995	9.616384	-0.051478	4.815499
246.564364	7999.872025	9.621389	-0.051460	4.815516
246.775943	7999.862687	9.626394	-0.051499	4.815512
246.777884	7999.875559	9.631399	-0.051500	4.815516
246.586860	7999.900233	9.636403	-0.051465	4.815524
246.853246	7999.845867	9.641408	-0.051515	4.815507
247.063819	7999.869620	9.646413	-0.051554	4.815513
246.849872	7999.826637	9.651418	-0.051515	4.815501
247.009252	7999.835671	9.656423	-0.051544	4.815503
246.874446	7999.921069	9.661427	-0.051520	4.815528
246.796809	7999.952933	9.666432	-0.051506	4.815538
246.868508	7999.945584	9.671437	-0.051519	4.815536
247.044041	7999.943134	9.676442	-0.051552	4.815534
247.174350	7999.889751	9.681447	-0.051577	4.815518
247.012003	7999.946932	9.686451	-0.051547	4.815535
247.012698	7999.934152	9.691456	-0.051547	4.815532
247.057901	7999.959478	9.696461	-0.051556	4.815539
247.025883	7999.899173	9.701466	-0.051550	4.815521
246.903704	7999.939922	9.706471	-0.051528	4.815534
247.156218	7999.971836	9.711475	-0.051575	4.815542
246.963131	7999.897154	9.716480	-0.051539	4.815521
247.010681	7999.910770	9.721485	-0.051548	4.815525
246.962859	7999.852344	9.726490	-0.051540	4.815508
247.061571	7999.836892	9.731495	-0.051558	4.815503
247.043326	7999.883609	9.736499	-0.051555	4.815517
247.024073	7999.903611	9.741504	-0.051552	4.815523
247.197222	7999.983357	9.746509	-0.051585	4.815545
246.800694	7999.911761	9.751514	-0.051511	4.815526
247.084521	7999.867292	9.756519	-0.051564	4.815512
247.020247	7999.868403	9.761523	-0.051552	4.815512
247.004730	7999.884194	9.766528	-0.051550	4.815517
247.267390	7999.973945	9.771533	-0.051599	4.815542
247.144286	7999.927104	9.776538	-0.051576	4.815529
247.259408	7999.916193	9.781543	-0.051598	4.815525
247.183421	7999.940608	9.786547	-0.051584	4.815532
247.049869	7999.922432	9.791552	-0.051560	4.815528
247.301697	7999.903073	9.796557	-0.051607	4.815521
247.044578	7999.911715	9.801562	-0.051559	4.815525
247.173345	7999.849763	9.806567	-0.051583	4.815506
247.251422	7999.936501	9.811571	-0.051598	4.815531
247.315318	7999.883101	9.816576	-0.051610	4.815515
247.407991	7999.931630	9.821581	-0.051628	4.815529
247.404629	7999.902764	9.826586	-0.051628	4.815520
247.511376	7999.919483	9.831591	-0.051648	4.815525
247.237883	7999.912906	9.836595	-0.051597	4.815524
247.271605	7999.917753	9.841600	-0.051604	4.815525
247.392038	7999.968872	9.846605	-0.051626	4.815540
247.399192	7999.907070	9.851610	-0.051628	4.815522
247.389678	7999.936842	9.856615	-0.051627	4.815530
247.150900	7999.959668	9.861619	-0.051582	4.815538
247.319673	7999.897301	9.866624	-0.051614	4.815519
247.252313	7999.949625	9.871629	-0.051602	4.815535
247.284388	7999.968329	9.876634	-0.051608	4.815540
247.307953	7999.978350	9.881639	-0.051613	4.815543
247.092594	7999.926799	9.886643	-0.051573	4.815529
247.343008	7999.862561	9.891648	-0.051620	4.815509
247.546594	7999.913969	9.896653	-0.051658	4.815523
247.398615	7999.945752	9.901658	-0.051631	4.815533
247.359663	7999.987860	9.906663	-0.051624	4.815545
247.442379	7999.931564	9.911667	-0.051639	4.815528
247.231232	7999.897169	9.916672	-0.051600	4.815519
247.404758	7999.966242	9.921677	-0.051633	4.815539
247.256030	7999.927527	9.926682	-0.051606	4.815528
247.352444	7999.909902	9.931687	-0.051624	4.815523
247.326579	7999.932999	9.936691	-0.051619	4.815529
247.288308	7999.930263	9.941696	-0.051612	4.815529
247.469608	7999.919364	9.946701	-0.051646	4.815525
247.415065	7999.880050	9.951706	-0.051637	4.815513
247.381715	7999.885938	9.956711	-0.051631	4.815515
247.462228	7999.920385	9.961715	-0.051646	4.815525
247.459416	7999.891528	9.966720	-0.051646	4.815517
247.404024	7999.952591	9.971725	-0.051636	4.815535
247.264790	7999.918302	9.976730	-0.051610	4.815525
247.360168	7999.949788	9.981735	-0.051628	4.815534
247.255312	7999.943828	9.986739	-0.051609	4.815533
247.207557	7999.896082	9.991744	-0.051600	4.815519
247.480209	7999.960365	9.996749	-0.051651	4.815537
247.456133	7999.921549	10.001754	-0.051647	4.815525
247.298726	7999.944635	10.006759	-0.051618	4.815533
247.291502	7999.926386	10.011763	-0.051617	4.815528
247.374675	7999.881845	10.016768	-0.051633	4.815514
247.474129	7999.953980	10.021773	-0.051651	4.815535
247.393438	7999.945211	10.026778	-0.051637	4.815532
247.422223	7999.953182	10.031783	-0.051642	4.815535
247.374839	7999.949229	10.036787	-0.051634	4.815534
247.451534	7999.914194	10.041792	-0.051648	4.815523
247.645862	7999.998559	10.046797	-0.051685	4.815547
247.588362	7999.920749	10.051802	-0.051674	4.815524
247.611698	7999.988438	10.056807	-0.051679	4.815544
247.498340	7999.994087	10.061811	-0.051658	4.815546
247.602400	7999.932799	10.066816	-0.051678	4.815528
247.542820	8000.000203	10.071821	-0.051667	4.815548
247.366229	7999.995207	10.076826	-0.051634	4.815547
247.475173	7999.998079	10.081831	-0.051655	4.815547
247.555416	7999.989802	10.086835	-0.051670	4.815545
247.416299	7999.982214	10.091840	-0.051645	4.815543
247.447726	7999.983820	10.096845	-0.051651	4.815543
247.514740	7999.900568	10.101850	-0.051663	4.815519
247.522227	7999.960522	10.106855	-0.051665	4.815536
247.431551	7999.952658	10.111859	-0.051649	4.815534
247.664133	7999.900944	10.116864	-0.051692	4.815518
247.704086	7999.966769	10.121869	-0.051700	4.815537
247.518607	7999.941337	10.126874	-0.051666	4.815531
247.542797	7999.959912	10.131879	-0.051670	4.815536
247.735020	7999.956668	10.136883	-0.051706	4.815534
247.600988	7999.880812	10.141888	-0.051682	4.815513
247.565536	7999.956085	10.146893	-0.051675	4.815535
247.738190	7999.945045	10.151898	-0.051708	4.815531
247.601804	7999.905462	10.156903	-0.051683	4.815520
247.539503	7999.941849	10.161907	-0.051671	4.815531
247.614758	7999.914267	10.166912	-0.051686	4.815522
247.649838	7999.890300	10.171917	-0.051693	4.815515
247.553272	7999.926128	10.176922	-0.051675	4.815526
247.706222	7999.915834	10.181927	-0.051704	4.815522
248.027518	7999.959554	10.186931	-0.051764	4.815533
247.873124	7999.952784	10.191936	-0.051735	4.815532
247.923668	7999.964315	10.196941	-0.051745	4.815535
247.795104	7999.957967	10.201946	-0.051721	4.815534
247.705921	7999.972555	10.206951	-0.051705	4.815539
247.555310	7999.970120	10.211955	-0.051677	4.815539
247.712325	7999.928921	10.216960	-0.051707	4.815526
247.999774	7999.964612	10.221965	-0.051761	4.815535
247.928929	7999.912215	10.226970	-0.051748	4.815520
247.913330	7999.981405	10.231975	-0.051745	4.815540
247.955027	7999.983179	10.236979	-0.051753	4.815541
247.893870	7999.924532	10.241984	-0.051742	4.815524
247.902432	7999.977028	10.246989	-0.051744	4.815539
247.873427	7999.931723	10.251994	-0.051739	4.815526
247.982109	7999.964495	10.256999	-0.051759	4.815535
247.893611	7999.948122	10.262003	-0.051743	4.815531
247.742020	7999.874114	10.267008	-0.051715	4.815510
248.147568	7999.888238	10.272013	-0.051791	4.815512
247.956940	7999.904373	10.277018	-0.051756	4.815518
248.063234	7999.945650	10.282023	-0.051776	4.815529
248.072877	7999.966124	10.287027	-0.051778	4.815535
247.812925	7999.945883	10.292032	-0.051730	4.815530
247.887517	7999.980234	10.297037	-0.051744	4.815540
247.887145	7999.927920	10.302042	-0.051744	4.815525
247.969260	7999.916469	10.307047	-0.051760	4.815521
247.813395	7999.933172	10.312051	-0.051731	4.815527
247.753163	7999.917261	10.317056	-0.051720	4.815522
247.954133	7999.945132	10.322061	-0.051758	4.815529
247.646454	7999.923043	10.327066	-0.051701	4.815524
247.696242	7999.948445	10.332071	-0.051710	4.815532
247.938101	7999.993004	10.337075	-0.051755	4.815543
247.900365	7999.927263	10.342080	-0.051749	4.815524
247.909615	7999.985111	10.347085	-0.051751	4.815541
247.772342	7999.966874	10.352090	-0.051725	4.815537
247.974303	7999.936020	10.357095	-0.051763	4.815527
247.907347	7999.925339	10.362099	-0.051751	4.815524
248.047555	7999.910566	10.367104	-0.051777	4.815519
248.070262	7999.955817	10.372109	-0.051782	4.815532
248.038698	7999.923286	10.377114	-0.051776	4.815523
248.254143	7999.894789	10.382119	-0.051817	4.815513
248.194450	7999.979280	10.387123	-0.051806	4.815538
247.991577	7999.923658	10.392128	-0.051768	4.815523
247.969432	7999.924389	10.397133	-0.051765	4.815523
247.871136	7999.900380	10.402138	-0.051747	4.815517
248.104714	7999.945871	10.407143	-0.051790	4.815529
247.811323	7999.973144	10.412147	-0.051736	4.815538
247.773935	7999.935178	10.417152	-0.051729	4.815527
247.929030	7999.993272	10.422157	-0.051759	4.815543
247.885647	7999.939187	10.427162	-0.051751	4.815528
247.840131	7999.933128	10.432167	-0.051742	4.815526
248.125671	7999.945293	10.437171	-0.051796	4.815528
248.164115	7999.865844	10.442176	-0.051803	4.815505
248.317171	7999.945266	10.447181	-0.051832	4.815528
248.055830	7999.895097	10.452186	-0.051784	4.815514
248.242272	7999.919527	10.457191	-0.051819	4.815520
248.236421	7999.942952	10.462195	-0.051818	4.815527
248.112636	7999.843766	10.467200	-0.051795	4.815499
248.121108	7999.891989	10.472205	-0.051797	4.815513
248.123060	7999.916609	10.477210	-0.051798	4.815520
248.174184	7999.919605	10.482215	-0.051807	4.815521
248.069571	7999.956369	10.487219	-0.051788	4.815532
248.032939	7999.889579	10.492224	-0.051782	4.815513
248.076140	7999.910601	10.497229	-0.051790	4.815518
247.987912	7999.884620	10.502234	-0.051774	4.815511
248.130620	7999.904064	10.507239	-0.051801	4.815516
248.383276	7999.917827	10.512243	-0.051848	4.815519
248.196090	7999.856054	10.517248	-0.051813	4.815502
248.214842	7999.923669	10.522253	-0.051817	4.815522
248.084389	7999.933311	10.527258	-0.051793	4.815525
247.985390	7999.945602	10.532263	-0.051775	4.815529
248.149826	7999.932292	10.537267	-0.051806	4.815524
248.236539	7999.849361	10.542272	-0.051822	4.815500
248.233110	7999.907001	10.547277	-0.051822	4.815517
248.080202	7999.924820	10.552282	-0.051794	4.815523
248.164184	7999.881360	10.557287	-0.051810	4.815509
248.327614	7999.945999	10.562291	-0.051841	4.815528
248.231462	7999.863284	10.567296	-0.051823	4.815504
248.322877	7999.979079	10.572301	-0.051840	4.815537
247.974847	7999.868754	10.577306	-0.051776	4.815507
248.055591	7999.822037	10.582311	-0.051791	4.815493
248.176732	7999.865692	10.587315	-0.051814	4.815505
248.127181	7999.852091	10.592320	-0.051805	4.815501
248.164619	7999.947780	10.597325	-0.051812	4.815529
248.054790	7999.895814	10.602330	-0.051792	4.815514
248.236662	7999.915897	10.607335	-0.051826	4.815519
248.213226	7999.948647	10.612339	-0.051822	4.815529
248.021774	7999.885736	10.617344	-0.051787	4.815511
248.178310	7999.936378	10.622349	-0.051816	4.815525
248.409518	7999.887846	10.627354	-0.051859	4.815510
248.400318	7999.880245	10.632359	-0.051858	4.815508
248.344129	7999.937024	10.637363	-0.051848	4.815525
248.251454	7999.878930	10.642368	-0.051831	4.815508
248.432732	7999.964153	10.647373	-0.051865	4.815532
248.221924	7999.914809	10.652378	-0.051826	4.815519
248.324734	7999.888744	10.657383	-0.051845	4.815511
248.180059	7999.941942	10.662387	-0.051819	4.815527
248.039156	7999.905489	10.667392	-0.051793	4.815517
248.292864	7999.978010	10.672397	-0.051840	4.815537
248.356270	7999.944894	10.677402	-0.051852	4.815527
248.160190	7999.976960	10.682407	-0.051816	4.815537
248.266626	7999.955227	10.687411	-0.051836	4.815530
248.409397	7999.904183	10.692416	-0.051863	4.815515
248.233163	7999.969681	10.697421	-0.051830	4.815535
248.093869	7999.900146	10.702426	-0.051805	4.815515
248.348119	7999.855195	10.707431	-0.051852	4.815501
248.482714	7999.962084	10.712435	-0.051878	4.815531
248.398460	7999.923351	10.717440	-0.051862	4.815520
248.392961	7999.936102	10.722445	-0.051862	4.815524
248.334597	7999.947989	10.727450	-0.051851	4.815528
248.328720	7999.911605	10.732455	-0.051850	4.815517
248.258373	7999.971357	10.737459	-0.051837	4.815535
248.377672	7999.949834	10.742464	-0.051860	4.815528
248.472002	7999.943924	10.747469	-0.051878	4.815526
248.385158	7999.941461	10.752474	-0.051862	4.815526
248.410717	7999.898115	10.757479	-0.051867	4.815513
248.257940	7999.953316	10.762483	-0.051839	4.815530
248.253642	7999.884917	10.767488	-0.051838	4.815510
248.416627	7999.986930	10.772493	-0.051869	4.815539
248.318327	7999.963988	10.777498	-0.051851	4.815532
248.304124	8000.001161	10.782503	-0.051848	4.815543
248.392604	7999.989815	10.787507	-0.051865	4.815540
248.556666	7999.971160	10.792512	-0.051896	4.815533
248.403642	7999.939847	10.797517	-0.051868	4.815525
248.145991	7999.943139	10.802522	-0.051820	4.815527
248.233595	7999.927506	10.807527	-0.051837	4.815522
248.389817	7999.963191	10.812531	-0.051866	4.815532
248.286084	7999.861128	10.817536	-0.051847	4.815503
248.298878	7999.954279	10.822541	-0.051850	4.815530
248.418001	7999.915664	10.827546	-0.051872	4.815518
248.708205	7999.898002	10.832551	-0.051926	4.815511
248.594644	7999.983749	10.837555	-0.051906	4.815537
248.463378	7999.933568	10.842560	-0.051881	4.815523
248.578407	7999.986737	10.847565	-0.051903	4.815538
248.539769	7999.939137	10.852570	-0.051896	4.815524
248.488003	7999.989581	10.857575	-0.051887	4.815539
248.617440	7999.953271	10.862579	-0.051911	4.815528
248.400226	7999.952951	10.867584	-0.051871	4.815529
248.635334	7999.980313	10.872589	-0.051915	4.815536
248.754985	7999.910735	10.877594	-0.051938	4.815515
248.797965	7999.905053	10.882599	-0.051946	4.815513
248.599658	7999.966987	10.887603	-0.051909	4.815532
248.624570	7999.943922	10.892608	-0.051914	4.815525
248.742005	7999.998199	10.897613	-0.051936	4.815540
248.382359	7999.943218	10.902618	-0.051870	4.815526
248.407750	7999.940453	10.907623	-0.051875	4.815525
248.477196	7999.955496	10.912627	-0.051888	4.815529
248.366446	7999.889630	10.917632	-0.051868	4.815510
248.278910	7999.927741	10.922637	-0.051852	4.815522
248.321550	7999.959435	10.927642	-0.051860	4.815531
248.413712	7999.951353	10.932647	-0.051877	4.815528
248.551376	7999.967511	10.937651	-0.051903	4.815532
248.559473	7999.913199	10.942656	-0.051905	4.815516
248.745099	7999.931208	10.947661	-0.051940	4.815521
248.555346	7999.936677	10.952666	-0.051905	4.815523
248.595827	7999.964063	10.957671	-0.051913	4.815531
248.530247	7999.896799	10.962675	-0.051901	4.815512
248.594555	7999.867969	10.967680	-0.051913	4.815503
248.686647	7999.932512	10.972685	-0.051930	4.815521
248.357277	7999.872686	10.977690	-0.051869	4.815505
248.497260	7999.847229	10.982695	-0.051895	4.815497
248.557328	7999.951833	10.987699	-0.051907	4.815528
248.396516	7999.937482	10.992704	-0.051877	4.815524
248.683460	7999.952875	10.997709	-0.051931	4.815527
248.392554	7999.899017	11.002714	-0.051877	4.815513
248.340541	7999.937709	11.007719	-0.051868	4.815524
248.569957	7999.974590	11.012723	-0.051911	4.815534
248.742877	7999.962488	11.017728	-0.051943	4.815530
248.688225	8000.006476	11.022733	-0.051933	4.815543
248.569343	7999.981062	11.027738	-0.051911	4.815536
248.659586	7999.922751	11.032743	-0.051929	4.815518
248.584359	8000.006989	11.037747	-0.051915	4.815543
248.381014	7999.966310	11.042752	-0.051877	4.815532
248.643041	7999.974888	11.047757	-0.051926	4.815534
248.559505	7999.985295	11.052762	-0.051911	4.815537
248.354162	7999.916815	11.057767	-0.051873	4.815518
248.312631	7999.909753	11.062771	-0.051866	4.815516
248.290138	7999.927567	11.067776	-0.051862	4.815522
248.642522	7999.988886	11.072781	-0.051928	4.815538
248.387958	7999.955914	11.077786	-0.051880	4.815529
248.595612	7999.930495	11.082791	-0.051919	4.815521
248.586565	7999.953868	11.087795	-0.051918	4.815528
248.352117	7999.929770	11.092800	-0.051875	4.815522
248.558656	7999.953461	11.097805	-0.051913	4.815528
248.514790	7999.939952	11.102810	-0.051905	4.815524
248.501604	7999.918401	11.107815	-0.051903	4.815518
248.628856	8000.004879	11.112819	-0.051927	4.815542
248.469840	7999.941428	11.117824	-0.051898	4.815525
248.558549	7999.984554	11.122829	-0.051915	4.815537
248.423637	7999.927905	11.127834	-0.051890	4.815521
248.580746	7999.994578	11.132839	-0.051919	4.815540
248.604734	8000.003539	11.137843	-0.051924	4.815542
248.484766	7999.966358	11.142848	-0.051902	4.815532
248.634240	7999.983778	11.147853	-0.051930	4.815536
248.547175	7999.932182	11.152858	-0.051914	4.815522
248.414610	7999.863824	11.157863	-0.051890	4.815502
248.500752	7999.944289	11.162867	-0.051906	4.815525
248.579345	7999.898604	11.167872	-0.051921	4.815512
248.621685	7999.970879	11.172877	-0.051929	4.815532
248.358769	7999.929226	11.177882	-0.051881	4.815522
248.631570	7999.935844	11.182887	-0.051932	4.815522
248.524989	7999.951216	11.187891	-0.051912	4.815527
248.715177	7999.915899	11.192896	-0.051948	4.815516
248.946744	8000.004082	11.197901	-0.051991	4.815541
248.735237	7999.930160	11.202906	-0.051952	4.815520
248.583197	7999.924496	11.207911	-0.051924	4.815519
248.621937	7999.977487	11.212915	-0.051932	4.815534
248.652964	7999.958794	11.217920	-0.051938	4.815529
248.726494	7999.967496	11.222925	-0.051952	4.815531
248.604636	7999.946305	11.227930	-0.051929	4.815525
248.843999	7999.955581	11.232935	-0.051974	4.815527
248.881336	7999.997869	11.237939	-0.051981	4.815539
248.651420	7999.914034	11.242944	-0.051939	4.815516
248.685287	7999.959469	11.247949	-0.051945	4.815529
248.634359	7999.942641	11.252954	-0.051936	4.815524
248.760024	7999.906269	11.257959	-0.051960	4.815513
248.602775	7999.959262	11.262963	-0.051931	4.815529
248.524703	7999.950534	11.267968	-0.051917	4.815527
248.917969	7999.985822	11.272973	-0.051990	4.815535
248.790157	7999.951717	11.277978	-0.051967	4.815526
248.720363	7999.898267	11.282983	-0.051954	4.815511
248.905080	8000.011318	11.287987	-0.051989	4.815543
248.786710	7999.966687	11.292992	-0.051967	4.815530
248.915613	8000.023288	11.297997	-0.051991	4.815546
248.870474	7999.991601	11.303002	-0.051983	4.815537
248.790924	7999.971101	11.308007	-0.051968	4.815532
248.600446	7999.989373	11.313011	-0.051933	4.815538
248.700797	7999.947248	11.318016	-0.051952	4.815525
248.721458	7999.963631	11.323021	-0.051956	4.815530
248.742440	7999.970407	11.328026	-0.051960	4.815532
248.777153	7999.931481	11.333031	-0.051967	4.815520
248.960886	7999.996454	11.338035	-0.052002	4.815538
248.644374	7999.952857	11.343040	-0.051943	4.815527
248.617611	8000.030411	11.348045	-0.051938	4.815550
248.680819	7999.926801	11.353050	-0.051950	4.815519
248.888393	7999.878952	11.358055	-0.051989	4.815504
248.895817	7999.942111	11.363059	-0.051991	4.815523
248.943853	7999.884179	11.368064	-0.052000	4.815505
248.780081	7999.966970	11.373069	-0.051970	4.815530
248.766446	7999.976384	11.378074	-0.051968	4.815533
248.778121	7999.895429	11.383079	-0.051970	4.815509
248.867504	8000.015466	11.388083	-0.051987	4.815544
248.764916	7999.990317	11.393088	-0.051968	4.815537
248.749398	7999.983680	11.398093	-0.051966	4.815535
248.722254	7999.990737	11.403098	-0.051961	4.815537
248.868169	7999.984601	11.408103	-0.051988	4.815535
248.877688	7999.987986	11.413107	-0.051990	4.815536
248.864296	7999.980315	11.418112	-0.051988	4.815534
248.863697	8000.030528	11.423117	-0.051988	4.815548
248.912002	7999.962987	11.428122	-0.051998	4.815528
248.744263	7999.996583	11.433127	-0.051967	4.815539
248.749800	7999.992426	11.438131	-0.051968	4.815538
248.670539	8000.001836	11.443136	-0.051954	4.815541
248.790025	8000.001677	11.448141	-0.051976	4.815540
248.997169	7999.942072	11.453146	-0.052015	4.815522
249.093430	7999.945806	11.458151	-0.052033	4.815523
248.884259	8000.005426	11.463155	-0.051994	4.815541
248.755182	7999.965960	11.468160	-0.051971	4.815530
248.955253	7999.973526	11.473165	-0.052008	4.815531
248.830532	7999.954424	11.478170	-0.051985	4.815526
248.781809	7999.973945	11.483175	-0.051976	4.815532
248.671040	7999.995656	11.488179	-0.051956	4.815539
248.803602	7999.942309	11.493184	-0.051981	4.815523
248.806947	7999.980837	11.498189	-0.051982	4.815534
248.809101	7999.940312	11.503194	-0.051983	4.815522
248.665922	7999.887799	11.508199	-0.051956	4.815508
248.815625	7999.959692	11.513203	-0.051984	4.815528
248.681698	7999.936167	11.518208	-0.051960	4.815522
248.876351	7999.987434	11.523213	-0.051996	4.815536
248.764713	7999.957865	11.528218	-0.051976	4.815528
248.806597	7999.921193	11.533223	-0.051984	4.815517
248.964226	7999.973991	11.538227	-0.052013	4.815531
248.777516	7999.978441	11.543232	-0.051979	4.815533
248.893563	8000.025220	11.548237	-0.052001	4.815547
248.995285	8000.040791	11.553242	-0.052020	4.815551
249.054450	7999.984108	11.558247	-0.052031	4.815534
248.996562	8000.024840	11.563251	-0.052021	4.815546
248.893255	7999.920645	11.568256	-0.052002	4.815516
249.035682	7999.990283	11.573261	-0.052029	4.815536
249.078053	8000.016633	11.578266	-0.052037	4.815543
248.914845	7999.975541	11.583271	-0.052007	4.815532
249.088132	8000.008303	11.588275	-0.052039	4.815541
248.807967	7999.962095	11.593280	-0.051987	4.815528
248.869487	7999.996234	11.598285	-0.051999	4.815538
248.883939	7999.960181	11.603290	-0.052002	4.815528
248.723138	7999.942625	11.608295	-0.051972	4.815523
248.961853	8000.002089	11.613299	-0.052017	4.815539
249.052078	7999.979023	11.618304	-0.052034	4.815532
249.220500	7999.987141	11.623309	-0.052066	4.815534
248.973668	7999.983131	11.628314	-0.052020	4.815534
248.716305	7999.963997	11.633319	-0.051973	4.815529
248.964272	8000.007591	11.638323	-0.052019	4.815541
248.935522	7999.956948	11.643328	-0.052014	4.815526
248.906337	7999.985332	11.648333	-0.052009	4.815535
248.867206	8000.018895	11.653338	-0.052002	4.815545
248.944021	8000.009494	11.658343	-0.052016	4.815542
248.865598	8000.003965	11.663347	-0.052002	4.815540
248.935579	7999.985908	11.668352	-0.052015	4.815535
249.094140	7999.952211	11.673357	-0.052045	4.815524
248.918159	7999.945087	11.678362	-0.052013	4.815523
248.926260	7999.919611	11.683367	-0.052014	4.815515
248.805570	7999.983882	11.688371	-0.051992	4.815535
249.002528	7999.967900	11.693376	-0.052029	4.815529
249.077603	7999.984104	11.698381	-0.052044	4.815533
248.968705	7999.935355	11.703386	-0.052023	4.815520
249.124366	7999.944332	11.708391	-0.052053	4.815522
249.266344	8000.000079	11.713395	-0.052080	4.815537
249.135886	7999.943501	11.718400	-0.052055	4.815521
249.161996	7999.952497	11.723405	-0.052061	4.815524
249.026785	7999.951379	11.728410	-0.052036	4.815524
248.976389	7999.969805	11.733415	-0.052027	4.815530
249.118865	7999.980702	11.738419	-0.052053	4.815532
249.141224	7999.871084	11.743424	-0.052058	4.815500
248.977882	8000.003012	11.748429	-0.052028	4.815539
248.916457	7999.998829	11.753434	-0.052017	4.815538
249.179243	8000.007421	11.758439	-0.052066	4.815540
249.255875	7999.983064	11.763443	-0.052080	4.815532
248.852679	7999.967955	11.768448	-0.052006	4.815530
249.086338	7999.975002	11.773453	-0.052049	4.815531
249.231995	7999.990224	11.778458	-0.052077	4.815534
249.094692	7999.958099	11.783463	-0.052051	4.815526
249.163469	8000.014786	11.788467	-0.052065	4.815542
249.113986	7999.967008	11.793472	-0.052056	4.815528
249.053249	7999.923318	11.798477	-0.052045	4.815516
248.845054	7999.958389	11.803482	-0.052006	4.815527
248.917618	7999.928626	11.808487	-0.052020	4.815518
249.297194	7999.967964	11.813491	-0.052091	4.815528
248.905584	7999.958384	11.818496	-0.052018	4.815527
248.957830	8000.007324	11.823501	-0.052028	4.815541
248.922089	7999.985403	11.828506	-0.052022	4.815534
248.951417	7999.943185	11.833511	-0.052028	4.815522
248.994202	7999.955658	11.838515	-0.052036	4.815525
249.106264	7999.913724	11.843520	-0.052057	4.815513
249.097917	7999.984103	11.848525	-0.052056	4.815533
248.846396	7999.980017	11.853530	-0.052009	4.815533
248.879979	7999.942140	11.858535	-0.052016	4.815522
249.066017	7999.984723	11.863539	-0.052051	4.815533
249.174122	8000.017488	11.868544	-0.052071	4.815542
249.149231	8000.047011	11.873549	-0.052067	4.815551
249.049225	8000.010155	11.878554	-0.052048	4.815541
248.832208	7999.915849	11.883559	-0.052008	4.815514
249.090651	7999.998065	11.888563	-0.052057	4.815537
248.959238	7999.944675	11.893568	-0.052032	4.815522
249.078511	7999.968010	11.898573	-0.052055	4.815528
249.038964	7999.970592	11.903578	-0.052048	4.815529
248.988077	7999.971921	11.908583	-0.052039	4.815530
249.142413	7999.985149	11.913587	-0.052068	4.815533
249.008785	7999.950948	11.918592	-0.052043	4.815524
249.027537	7999.981184	11.923597	-0.052047	4.815532
249.052715	7999.949578	11.928602	-0.052052	4.815523
248.983322	7999.931380	11.933607	-0.052039	4.815518
249.095103	7999.991974	11.938611	-0.052060	4.815535
249.213354	7999.977911	11.943616	-0.052082	4.815531
249.333106	7999.984165	11.948621	-0.052105	4.815532
248.988777	7999.983901	11.953626	-0.052041	4.815533
248.996691	7999.929585	11.958631	-0.052043	4.815518
249.117046	7999.965754	11.963635	-0.052066	4.815528
248.961304	7999.947212	11.968640	-0.052037	4.815523
249.251908	7999.934898	11.973645	-0.052091	4.815518
249.183903	7999.931675	11.978650	-0.052079	4.815517
249.119327	7999.937052	11.983655	-0.052067	4.815519
249.060256	8000.023691	11.988659	-0.052056	4.815545
248.972128	7999.953920	11.993664	-0.052040	4.815525
249.126640	7999.999192	11.998669	-0.052069	4.815537
248.987369	7999.998008	12.003674	-0.052044	4.815537
248.865028	7999.957583	12.008679	-0.052021	4.815526
249.019199	7999.995373	12.013683	-0.052050	4.815537
249.073238	7999.981328	12.018688	-0.052061	4.815532
249.095654	8000.005216	12.023693	-0.052065	4.815539
249.126427	7999.984383	12.028698	-0.052071	4.815533
249.124262	7999.980099	12.033703	-0.052071	4.815532
249.197769	8000.017639	12.038707	-0.052085	4.815542
249.179359	7999.969300	12.043712	-0.052082	4.815528
249.220438	8000.042624	12.048717	-0.052090	4.815549
248.973569	8000.019388	12.053722	-0.052044	4.815544
249.032380	7999.944543	12.058727	-0.052055	4.815522
249.233638	8000.032233	12.063731	-0.052093	4.815546
249.051973	7999.965205	12.068736	-0.052059	4.815528
249.061567	7999.962182	12.073741	-0.052061	4.815527
249.154190	7999.994694	12.078746	-0.052079	4.815536
248.996139	7999.909895	12.083751	-0.052050	4.815512
249.083198	8000.020284	12.088755	-0.052066	4.815543
249.160885	7999.978856	12.093760	-0.052081	4.815531
249.277879	8000.002154	12.098765	-0.052103	4.815537
249.175838	8000.007987	12.103770	-0.052084	4.815539
249.153629	7999.989491	12.108775	-0.052081	4.815534
249.293897	8000.002489	12.113779	-0.052107	4.815537
249.003066	7999.979603	12.118784	-0.052053	4.815532
249.093402	7999.991784	12.123789	-0.052070	4.815535
249.231851	7999.963098	12.128794	-0.052096	4.815526
249.348246	7999.932984	12.133799	-0.052118	4.815517
249.198815	7999.997853	12.138803	-0.052091	4.815536
249.081938	7999.900911	12.143808	-0.052069	4.815508
249.229675	7999.935392	12.148813	-0.052097	4.815518
249.463706	7999.956330	12.153818	-0.052141	4.815523
249.266753	7999.968088	12.158823	-0.052104	4.815527
249.225364	7999.980253	12.163827	-0.052097	4.815531
249.210023	7999.945849	12.168832	-0.052094	4.815521
249.269055	7999.994901	12.173837	-0.052106	4.815535
249.299101	7999.912108	12.178842	-0.052111	4.815511
249.332437	7999.892385	12.183847	-0.052118	4.815505
249.432089	7999.997639	12.188851	-0.052137	4.815535
249.223414	7999.945122	12.193856	-0.052098	4.815521
249.306963	8000.025548	12.198861	-0.052114	4.815544
249.284466	8000.007048	12.203866	-0.052110	4.815538
249.061829	7999.984208	12.208871	-0.052069	4.815533
249.159781	8000.036032	12.213875	-0.052088	4.815547
249.138426	7999.998326	12.218880	-0.052084	4.815537
249.201783	7999.956664	12.223885	-0.052096	4.815524
249.217867	7999.978312	12.228890	-0.052099	4.815530
249.186684	7999.896655	12.233895	-0.052094	4.815507
249.414389	7999.958077	12.238899	-0.052136	4.815523
249.303938	7999.956296	12.243904	-0.052116	4.815523
249.388740	7999.985476	12.248909	-0.052132	4.815532
249.426230	8000.006406	12.253914	-0.052139	4.815537
249.148078	7999.894011	12.258919	-0.052088	4.815506
249.369160	7999.999114	12.263923	-0.052129	4.815536
249.336416	7999.996467	12.268928	-0.052124	4.815535
249.452385	8000.005864	12.273933	-0.052145	4.815537
249.142947	7999.992285	12.278938	-0.052088	4.815535
249.378384	7999.992954	12.283943	-0.052132	4.815534
249.363042	8000.010885	12.288947	-0.052130	4.815539
249.262082	7999.939836	12.293952	-0.052111	4.815519
249.222127	7999.984065	12.298957	-0.052104	4.815532
249.212732	7999.994617	12.303962	-0.052102	4.815535
249.322653	7999.935559	12.308967	-0.052123	4.815517
249.435006	7999.929944	12.313971	-0.052144	4.815515
249.206411	7999.925163	12.318976	-0.052102	4.815515
249.269058	7999.951845	12.323981	-0.052114	4.815522
249.254978	8000.006110	12.328986	-0.052112	4.815538
249.359652	7999.979008	12.333991	-0.052131	4.815530
249.488954	8000.018529	12.338995	-0.052156	4.815541
249.422372	7999.923476	12.344000	-0.052144	4.815513
249.347762	7999.936165	12.349005	-0.052130	4.815517
249.400540	7999.960550	12.354010	-0.052140	4.815524
249.400251	7999.981931	12.359015	-0.052140	4.815530
249.522671	8000.041632	12.364019	-0.052164	4.815547
249.595576	8000.019351	12.369024	-0.052177	4.815540
249.374960	8000.025381	12.374029	-0.052137	4.815543
249.355778	8000.032569	12.379034	-0.052133	4.815545
249.253905	7999.990341	12.384039	-0.052115	4.815533
249.392002	7999.994760	12.389043	-0.052141	4.815534
249.175989	7999.958143	12.394048	-0.052101	4.815524
249.262007	7999.976663	12.399053	-0.052117	4.815529
249.312521	8000.026643	12.404058	-0.052127	4.815544
249.191921	8000.005471	12.409063	-0.052104	4.815538
249.266626	8000.015262	12.414067	-0.052119	4.815541
249.251344	7999.941340	12.419072	-0.052116	4.815519
249.257012	7999.974567	12.424077	-0.052117	4.815529
249.311923	7999.980830	12.429082	-0.052128	4.815530
249.247923	7999.986216	12.434087	-0.052116	4.815532
249.558718	8000.036181	12.439091	-0.052174	4.815545
249.445988	7999.989503	12.444096	-0.052154	4.815532
249.516366	7999.947956	12.449101	-0.052167	4.815520
249.498929	7999.973329	12.454106	-0.052164	4.815527
249.354991	7999.950707	12.459111	-0.052138	4.815521
249.419172	7999.995571	12.464115	-0.052150	4.815534
249.372604	7999.975609	12.469120	-0.052141	4.815528
249.452174	8000.039950	12.474125	-0.052157	4.815547
249.308225	8000.050438	12.479130	-0.052130	4.815551
249.200521	7999.989958	12.484135	-0.052110	4.815533
249.470545	8000.011486	12.489139	-0.052161	4.815538
249.337655	7999.991181	12.494144	-0.052136	4.815533
249.274059	7999.985894	12.499149	-0.052125	4.815532
249.399948	7999.967683	12.504154	-0.052148	4.815526
249.273865	7999.888747	12.509159	-0.052125	4.815503
249.601695	7999.966758	12.514163	-0.052187	4.815525
249.676029	7999.962658	12.519168	-0.052201	4.815523
249.745281	7999.965951	12.524173	-0.052214	4.815524
249.655201	8000.005089	12.529178	-0.052197	4.815536
249.412583	7999.972309	12.534183	-0.052152	4.815527
249.480416	7999.984123	12.539187	-0.052165	4.815530
249.409238	7999.996869	12.544192	-0.052152	4.815534
249.554588	7999.987521	12.549197	-0.052180	4.815531
249.595323	8000.002096	12.554202	-0.052188	4.815535
249.568485	7999.996342	12.559207	-0.052183	4.815533
249.501439	8000.033720	12.564211	-0.052171	4.815545
249.486446	8000.034568	12.569216	-0.052168	4.815545
249.579952	8000.061755	12.574221	-0.052186	4.815552
249.524312	8000.021351	12.579226	-0.052176	4.815541
249.295800	8000.022980	12.584231	-0.052134	4.815542
249.593455	8000.039620	12.589235	-0.052189	4.815546
249.431808	8000.009231	12.594240	-0.052159	4.815538
249.328123	7999.975519	12.599245	-0.052140	4.815528
249.443613	8000.024426	12.604250	-0.052162	4.815542
249.549281	7999.945006	12.609255	-0.052182	4.815518
249.487419	8000.020919	12.614259	-0.052171	4.815541
249.542225	7999.997274	12.619264	-0.052181	4.815534
249.610440	7999.974917	12.624269	-0.052194	4.815527
249.593602	8000.001368	12.629274	-0.052191	4.815535
249.619913	7999.990073	12.634279	-0.052197	4.815531
249.740272	8000.002747	12.639283	-0.052219	4.815534
249.725985	7999.958747	12.644288	-0.052217	4.815522
249.602414	8000.008018	12.649293	-0.052194	4.815537
249.567698	8000.014951	12.654298	-0.052188	4.815539
249.738751	7999.990003	12.659303	-0.052220	4.815531
249.658774	7999.964154	12.664307	-0.052206	4.815523
249.602618	7999.951512	12.669312	-0.052195	4.815520
249.749129	8000.007335	12.674317	-0.052223	4.815536
249.919440	7999.999464	12.679322	-0.052255	4.815532
249.708532	7999.963998	12.684327	-0.052216	4.815523
249.805590	8000.016877	12.689331	-0.052234	4.815538
249.812348	7999.978561	12.694336	-0.052236	4.815527
249.714378	8000.011162	12.699341	-0.052218	4.815537
249.495094	8000.025758	12.704346	-0.052177	4.815542
249.434896	7999.992756	12.709351	-0.052166	4.815533
249.363722	8000.049292	12.714355	-0.052153	4.815550
249.504843	7999.930933	12.719360	-0.052180	4.815514
249.408875	7999.967839	12.724365	-0.052162	4.815526
249.611488	7999.982925	12.729370	-0.052200	4.815529
249.436263	7999.976880	12.734375	-0.052168	4.815528
249.695065	8000.008906	12.739379	-0.052217	4.815536
249.504522	7999.970569	12.744384	-0.052181	4.815526
249.561836	8000.038818	12.749389	-0.052192	4.815546
249.594596	8000.041515	12.754394	-0.052199	4.815546
249.495035	7999.959806	12.759399	-0.052180	4.815523
249.525172	8000.000910	12.764403	-0.052186	4.815535
249.333754	7999.943334	12.769408	-0.052151	4.815519
249.576485	7999.978301	12.774413	-0.052196	4.815528
249.677267	7999.985313	12.779418	-0.052215	4.815529
249.448417	7999.978392	12.784423	-0.052173	4.815528
249.654155	8000.036252	12.789427	-0.052212	4.815544
249.546728	7999.993933	12.794432	-0.052192	4.815532
249.599446	7999.983071	12.799437	-0.052202	4.815529
249.679416	8000.000424	12.804442	-0.052217	4.815534
249.649839	7999.954038	12.809447	-0.052212	4.815520
249.715236	8000.040577	12.814451	-0.052224	4.815545
249.509735	7999.972089	12.819456	-0.052186	4.815526
249.711828	7999.978622	12.824461	-0.052224	4.815527
249.596572	8000.017349	12.829466	-0.052203	4.815539
249.475803	7999.947043	12.834471	-0.052181	4.815519
249.605109	7999.992972	12.839475	-0.052205	4.815532
249.578930	7999.963731	12.844480	-0.052201	4.815523
249.514788	7999.949890	12.849485	-0.052189	4.815520
249.703606	7999.983975	12.854490	-0.052225	4.815529
249.808354	7999.928037	12.859495	-0.052244	4.815512
249.699558	7999.955120	12.864499	-0.052224	4.815520
249.649730	7999.960738	12.869504	-0.052215	4.815522
249.705105	7999.976621	12.874509	-0.052226	4.815527
249.823574	8000.020238	12.879514	-0.052248	4.815539
249.502384	7999.906068	12.884519	-0.052189	4.815507
249.442475	8000.000170	12.889523	-0.052178	4.815535
249.548630	7999.938915	12.894528	-0.052198	4.815516
249.532394	7999.883134	12.899533	-0.052195	4.815500
249.481706	7999.940006	12.904538	-0.052186	4.815517
249.448723	7999.930946	12.909543	-0.052180	4.815514
249.707547	8000.008899	12.914547	-0.052229	4.815536
249.534975	7999.993285	12.919552	-0.052197	4.815532
249.682447	7999.931637	12.924557	-0.052224	4.815513
249.687394	7999.991554	12.929562	-0.052226	4.815531
249.638726	7999.927767	12.934567	-0.052217	4.815513
249.721473	8000.027407	12.939571	-0.052233	4.815541
249.520030	8000.004912	12.944576	-0.052195	4.815536
249.556487	7999.991648	12.949581	-0.052202	4.815532
249.536988	7999.999898	12.954586	-0.052199	4.815534
249.629300	7999.949097	12.959591	-0.052217	4.815519
249.715363	7999.962277	12.964595	-0.052233	4.815522
249.536022	7999.979662	12.969600	-0.052200	4.815528
249.582015	7999.951601	12.974605	-0.052209	4.815520
249.445756	7999.957942	12.979610	-0.052183	4.815522
249.469542	7999.890000	12.984615	-0.052188	4.815502
249.555253	7999.973666	12.989619	-0.052204	4.815526
249.597466	7999.985062	12.994624	-0.052213	4.815529
249.805707	7999.956449	12.999629	-0.052252	4.815520
249.702625	8000.042370	13.004634	-0.052233	4.815546
249.570764	8000.012469	13.009639	-0.052208	4.815537
249.603412	8000.047205	13.014643	-0.052215	4.815547
249.506912	7999.966615	13.019648	-0.052197	4.815524
249.575928	7999.977380	13.024653	-0.052210	4.815527
249.652007	7999.991465	13.029658	-0.052225	4.815531
249.425167	7999.941854	13.034663	-0.052183	4.815518
249.424436	7999.977113	13.039667	-0.052183	4.815528
249.578397	7999.984995	13.044672	-0.052212	4.815529
249.552177	7999.960025	13.049677	-0.052207	4.815522
249.472144	7999.980102	13.054682	-0.052193	4.815528
249.482079	7999.954656	13.059687	-0.052195	4.815521
249.598762	7999.999311	13.064691	-0.052217	4.815533
249.533205	8000.015353	13.069696	-0.052205	4.815538
249.310044	7999.992503	13.074701	-0.052164	4.815533
249.501318	8000.028765	13.079706	-0.052199	4.815542
249.350314	7999.981462	13.084711	-0.052172	4.815529
249.455444	8000.018451	13.089715	-0.052191	4.815540
249.535489	7999.969585	13.094720	-0.052207	4.815525
249.537142	7999.922642	13.099725	-0.052207	4.815511
249.650996	7999.959774	13.104730	-0.052229	4.815522
249.597564	7999.932223	13.109735	-0.052219	4.815514
249.536461	7999.978244	13.114739	-0.052208	4.815528
249.617079	7999.982791	13.119744	-0.052223	4.815528
249.580746	7999.965132	13.124749	-0.052217	4.815523
249.564394	8000.009748	13.129754	-0.052214	4.815537
249.612689	7999.975316	13.134759	-0.052223	4.815526
249.704927	8000.028116	13.139763	-0.052241	4.815541
249.676958	8000.000982	13.144768	-0.052236	4.815533
249.728591	7999.948447	13.149773	-0.052246	4.815518
249.801278	7999.958204	13.154778	-0.052259	4.815520
249.709180	7999.892639	13.159783	-0.052243	4.815502
249.848370	7999.981453	13.164787	-0.052269	4.815527
249.700627	7999.975857	13.169792	-0.052242	4.815526
249.752880	7999.925469	13.174797	-0.052252	4.815511
249.792436	7999.969931	13.179802	-0.052259	4.815524
249.626598	7999.909568	13.184807	-0.052229	4.815507
249.626541	7999.969404	13.189811	-0.052229	4.815524
249.503639	7999.984508	13.194816	-0.052206	4.815529
249.859465	7999.945491	13.199821	-0.052273	4.815516
249.879112	8000.004581	13.204826	-0.052277	4.815533
249.681552	7999.875343	13.209831	-0.052240	4.815497
249.808498	7999.989591	13.214835	-0.052264	4.815529
249.602563	7999.947797	13.219840	-0.052226	4.815518
249.842147	7999.931446	13.224845	-0.052271	4.815512
249.724810	7999.980819	13.229850	-0.052249	4.815527
249.698503	7999.920601	13.234855	-0.052245	4.815510
249.871259	7999.985399	13.239859	-0.052277	4.815528
249.841565	7999.942215	13.244864	-0.052272	4.815515
249.928032	7999.922292	13.249869	-0.052288	4.815509
249.825448	7999.940932	13.254874	-0.052269	4.815515
249.727055	7999.892353	13.259879	-0.052251	4.815501
249.869958	7999.960934	13.264883	-0.052278	4.815521
249.998497	7999.956653	13.269888	-0.052303	4.815519
249.582879	7999.949881	13.274893	-0.052225	4.815519
249.658194	8000.002404	13.279898	-0.052240	4.815534
249.698524	7999.967842	13.284903	-0.052248	4.815523
249.775456	8000.015052	13.289907	-0.052262	4.815537
249.531300	7999.980109	13.294912	-0.052217	4.815528
249.729422	8000.020756	13.299917	-0.052254	4.815539
249.643338	8000.010828	13.304922	-0.052238	4.815536
249.520791	7999.961854	13.309927	-0.052216	4.815523
249.694449	7999.993556	13.314931	-0.052248	4.815531
249.707045	7999.948927	13.319936	-0.052251	4.815518
249.620156	7999.921897	13.324941	-0.052235	4.815510
249.792092	7999.981341	13.329946	-0.052267	4.815527
249.799684	7999.839436	13.334951	-0.052269	4.815485
249.916127	7999.885156	13.339955	-0.052291	4.815498
249.754413	7999.933803	13.344960	-0.052261	4.815513
249.874876	7999.924049	13.349965	-0.052284	4.815510
249.921019	7999.950462	13.354970	-0.052293	4.815517
249.697510	7999.914789	13.359975	-0.052252	4.815508
249.740266	7999.920853	13.364979	-0.052260	4.815509
249.787550	7999.890677	13.369984	-0.052269	4.815500
249.884522	7999.923261	13.374989	-0.052287	4.815509
249.711071	7999.994146	13.379994	-0.052255	4.815531
249.757696	7999.905215	13.384999	-0.052264	4.815505
249.922997	7999.914351	13.390003	-0.052295	4.815507
249.713126	7999.934441	13.395008	-0.052256	4.815513
249.840921	8000.015593	13.400013	-0.052281	4.815537
249.979613	7999.984775	13.405018	-0.052307	4.815527
249.847059	7999.958066	13.410023	-0.052282	4.815520
249.782326	8000.008300	13.415027	-0.052270	4.815535
249.816859	7999.990732	13.420032	-0.052277	4.815529
249.861482	7999.949831	13.425037	-0.052286	4.815517
249.715767	7999.970970	13.430042	-0.052259	4.815524
249.821518	7999.920389	13.435047	-0.052279	4.815509
249.810541	7999.949071	13.440051	-0.052277	4.815517
249.914294	7999.930499	13.445056	-0.052297	4.815511
250.013923	7999.915064	13.450061	-0.052315	4.815506
250.039085	7999.940065	13.455066	-0.052320	4.815513
249.832447	7999.882239	13.460071	-0.052282	4.815498
249.780019	7999.934810	13.465075	-0.052273	4.815513
249.854053	7999.896526	13.470080	-0.052287	4.815502
249.733719	7999.911672	13.475085	-0.052265	4.815507
249.654394	7999.909332	13.480090	-0.052250	4.815506
249.612657	7999.886244	13.485095	-0.052243	4.815500
250.024141	7999.993397	13.490099	-0.052320	4.815529
249.812428	8000.000640	13.495104	-0.052280	4.815532
249.601168	8000.013230	13.500109	-0.052241	4.815537
249.777659	8000.028958	13.505114	-0.052275	4.815541
249.759346	7999.907991	13.510119	-0.052271	4.815505
249.901413	7999.908202	13.515123	-0.052298	4.815505
250.088229	7999.945460	13.520128	-0.052333	4.815515
249.778125	7999.987409	13.525133	-0.052276	4.815528
249.641912	8000.010839	13.530138	-0.052251	4.815536
249.692227	7999.982849	13.535143	-0.052260	4.815528
249.674236	7999.994328	13.540147	-0.052257	4.815531
249.587867	7999.908562	13.545152	-0.052241	4.815506
249.733034	7999.906688	13.550157	-0.052269	4.815505
249.750690	8000.003128	13.555162	-0.052272	4.815533
249.823732	7999.926378	13.560167	-0.052286	4.815510
249.777382	7999.949142	13.565171	-0.052278	4.815517
249.920763	7999.970736	13.570176	-0.052305	4.815523
249.970704	7999.937399	13.575181	-0.052314	4.815513
249.780686	7999.981312	13.580186	-0.052279	4.815527
249.974564	7999.917218	13.585191	-0.052316	4.815507
250.156185	7999.978957	13.590195	-0.052350	4.815524
249.778287	7999.966393	13.595200	-0.052280	4.815522
249.815343	7999.924300	13.600205	-0.052287	4.815510
249.918767	7999.977284	13.605210	-0.052306	4.815525
249.786599	7999.915335	13.610215	-0.052282	4.815507
249.529510	7999.930381	13.615219	-0.052234	4.815513
249.553984	7999.957507	13.620224	-0.052239	4.815521
249.727499	7999.955028	13.625229	-0.052272	4.815519
249.691500	7999.976894	13.630234	-0.052265	4.815526
249.625726	7999.965162	13.635239	-0.052254	4.815523
249.866327	8000.009708	13.640243	-0.052299	4.815534
249.876966	7999.955435	13.645248	-0.052301	4.815518
249.759932	7999.925775	13.650253	-0.052279	4.815510
249.941467	7999.959743	13.655258	-0.052313	4.815519
249.828805	7999.946176	13.660263	-0.052293	4.815516
249.912622	7999.949707	13.665267	-0.052309	4.815517
249.896832	7999.961222	13.670272	-0.052306	4.815520
249.851536	7999.929532	13.675277	-0.052298	4.815511
249.790111	7999.970207	13.680282	-0.052287	4.815523
249.737491	7999.912763	13.685287	-0.052277	4.815507
249.880731	7999.967466	13.690291	-0.052304	4.815522
249.807704	7999.947070	13.695296	-0.052291	4.815516
249.677751	7999.933221	13.700301	-0.052267	4.815513
249.989522	7999.973591	13.705306	-0.052325	4.815523
249.765392	7999.943248	13.710311	-0.052284	4.815515
249.817601	7999.950534	13.715315	-0.052294	4.815517
249.699639	7999.946494	13.720320	-0.052272	4.815517
249.817876	7999.951656	13.725325	-0.052294	4.815518
249.890178	8000.004131	13.730330	-0.052308	4.815532
249.649484	7999.983130	13.735335	-0.052264	4.815528
249.818826	8000.027579	13.740339	-0.052295	4.815540
249.785795	8000.017450	13.745344	-0.052289	4.815537
249.899821	8000.005455	13.750349	-0.052311	4.815533
249.934246	7999.988953	13.755354	-0.052318	4.815528
249.772325	7999.916904	13.760359	-0.052288	4.815508
250.018283	7999.965810	13.765363	-0.052334	4.815521
249.981594	7999.959894	13.770368	-0.052327	4.815519
249.992297	7999.954753	13.775373	-0.052330	4.815518
249.978389	8000.004750	13.780378	-0.052327	4.815532
249.746568	7999.956124	13.785383	-0.052284	4.815519
250.075213	7999.980749	13.790387	-0.052346	4.815525
250.007841	8000.013850	13.795392	-0.052334	4.815535
249.760291	7999.983124	13.800397	-0.052288	4.815527
249.757450	8000.022621	13.805402	-0.052288	4.815538
249.891026	7999.993856	13.810407	-0.052313	4.815529
249.854488	7999.997555	13.815411	-0.052306	4.815531
249.836979	7999.953502	13.820416	-0.052303	4.815518
249.955754	7999.939448	13.825421	-0.052326	4.815513
250.170361	8000.000659	13.830426	-0.052366	4.815530
249.947062	7999.957512	13.835431	-0.052325	4.815518
249.993845	7999.973255	13.840435	-0.052334	4.815523
250.168326	7999.971861	13.845440	-0.052366	4.815522
249.958634	7999.985545	13.850445	-0.052328	4.815527
249.818363	7999.985411	13.855450	-0.052302	4.815527
250.037360	7999.952703	13.860455	-0.052343	4.815517
250.152056	7999.988782	13.865459	-0.052364	4.815527
249.959815	8000.009160	13.870464	-0.052329	4.815533
250.068863	7999.944747	13.875469	-0.052349	4.815514
249.953099	7999.994146	13.880474	-0.052328	4.815529
249.838703	7999.944236	13.885479	-0.052307	4.815515
250.074500	7999.962002	13.890483	-0.052351	4.815519
249.981436	7999.955164	13.895488	-0.052334	4.815518
250.091566	7999.970875	13.900493	-0.052355	4.815522
249.864075	7999.957566	13.905498	-0.052313	4.815519
249.978824	7999.933833	13.910503	-0.052335	4.815511
250.188637	7999.965059	13.915507	-0.052374	4.815519
250.132499	7999.954553	13.920512	-0.052364	4.815517
250.072941	7999.955739	13.925517	-0.052353	4.815517
250.299289	8000.031028	13.930522	-0.052395	4.815538
250.109734	7999.949982	13.935527	-0.052360	4.815515
250.195831	7999.961027	13.940531	-0.052377	4.815518
249.935927	7999.934371	13.945536	-0.052329	4.815512
249.928665	7999.904371	13.950541	-0.052327	4.815503
249.884755	7999.963490	13.955546	-0.052320	4.815520
249.970002	7999.962772	13.960551	-0.052336	4.815520
250.040193	7999.982102	13.965555	-0.052349	4.815525
250.204607	7999.990156	13.970560	-0.052380	4.815527
250.150767	7999.959394	13.975565	-0.052370	4.815518
250.161118	8000.009788	13.980570	-0.052372	4.815532
250.226466	8000.005541	13.985575	-0.052385	4.815531
250.266939	8000.064972	13.990579	-0.052393	4.815548
250.032686	8000.007760	13.995584	-0.052349	4.815532
250.035255	7999.945878	14.000589	-0.052350	4.815514
249.922555	7999.957944	14.005594	-0.052329	4.815518
249.989674	7999.956930	14.010599	-0.052342	4.815518
250.032539	8000.021741	14.015603	-0.052351	4.815537
249.859713	7999.981556	14.020608	-0.052319	4.815526
250.025152	7999.988559	14.025613	-0.052350	4.815527
249.994355	8000.021190	14.030618	-0.052344	4.815537
249.760494	7999.896697	14.035623	-0.052301	4.815501
249.977976	7999.997473	14.040627	-0.052342	4.815530
249.869055	7999.992512	14.045632	-0.052322	4.815529
249.932574	7999.964737	14.050637	-0.052334	4.815520
249.936600	8000.040662	14.055642	-0.052335	4.815542
249.857110	7999.988118	14.060647	-0.052320	4.815528
249.958584	8000.021845	14.065651	-0.052340	4.815537
249.930877	7999.987237	14.070656	-0.052335	4.815527
249.950351	7999.968355	14.075661	-0.052339	4.815521
250.139061	7999.966125	14.080666	-0.052374	4.815520
249.863454	7999.912510	14.085671	-0.052323	4.815505
250.056198	8000.029972	14.090675	-0.052359	4.815539
249.991599	8000.011851	14.095680	-0.052347	4.815534
249.939201	8000.108214	14.100685	-0.052338	4.815562
249.761061	8000.089304	14.105690	-0.052305	4.815557
249.662080	8000.006535	14.110695	-0.052287	4.815534
249.753151	8000.056113	14.115699	-0.052304	4.815548
249.762307	8000.021040	14.120704	-0.052306	4.815537
249.796328	7999.977830	14.125709	-0.052313	4.815525
249.748364	7999.997363	14.130714	-0.052304	4.815531
249.541812	7999.997214	14.135719	-0.052266	4.815532
249.615465	8000.023009	14.140723	-0.052280	4.815539
249.664979	7999.991801	14.145728	-0.052289	4.815529
249.581212	7999.971230	14.150733	-0.052274	4.815524
249.678322	8000.024110	14.155738	-0.052292	4.815539
249.623083	7999.981576	14.160743	-0.052282	4.815527
249.702904	7999.959408	14.165747	-0.052297	4.815520
249.696181	7999.970004	14.170752	-0.052296	4.815523
249.696191	7999.965756	14.175757	-0.052297	4.815522
249.866701	7999.998476	14.180762	-0.052329	4.815530
249.721682	7999.955541	14.185767	-0.052302	4.815518
249.793142	7999.926828	14.190771	-0.052316	4.815510
249.766457	7999.929620	14.195776	-0.052311	4.815511
249.936413	7999.933493	14.200781	-0.052343	4.815511
249.877155	7999.998769	14.205786	-0.052332	4.815530
249.901872	7999.971428	14.210791	-0.052337	4.815522
250.004570	7999.999834	14.215795	-0.052356	4.815530
249.950499	7999.968000	14.220800	-0.052347	4.815521
249.836084	7999.923430	14.225805	-0.052326	4.815508
249.893745	7999.697965	14.230810	-0.052336	4.815442

249.921277	7996.366408	14.235815	-0.052340	4.814468
250.070908	7990.807355	14.240819	-0.052364	4.812842
249.930592	7983.978875	14.245824	-0.052334	4.810845
249.992759	7976.649852	14.250829	-0.052341	4.808700
249.871376	7969.022718	14.255834	-0.052314	4.806467
249.714062	7961.197232	14.260839	-0.052280	4.804176
249.718266	7953.430194	14.265843	-0.052276	4.801900
249.655871	7945.379484	14.270848	-0.052259	4.799539
249.741421	7937.455194	14.275853	-0.052270	4.797214
249.754067	7929.394336	14.280858	-0.052267	4.794849
249.493084	7921.389842	14.285863	-0.052214	4.792499
249.300890	7913.342553	14.290867	-0.052173	4.790136
249.366168	7905.379394	14.295872	-0.052180	4.787795
249.544099	7897.333581	14.300877	-0.052209	4.785428
249.420261	7889.449874	14.305882	-0.052181	4.783109
249.122258	7881.423489	14.310887	-0.052120	4.780748
249.381142	7873.422371	14.315891	-0.052163	4.778390
249.317366	7865.414529	14.320896	-0.052147	4.776031
249.200936	7857.352824	14.325901	-0.052120	4.773655
249.322951	7849.422030	14.330906	-0.052138	4.771315
249.280007	7841.315327	14.335911	-0.052125	4.768923
249.289253	7833.402595	14.340915	-0.052122	4.766587
249.159765	7825.329337	14.345920	-0.052093	4.764203
249.209382	7817.409119	14.350925	-0.052097	4.761862
249.195123	7809.363250	14.355930	-0.052089	4.759483
249.006007	7801.364766	14.360935	-0.052049	4.757117
249.127221	7793.370701	14.365939	-0.052067	4.754751
248.951022	7785.289775	14.370944	-0.052029	4.752358
248.936307	7777.299043	14.375949	-0.052021	4.749991
248.785755	7769.345594	14.380954	-0.051988	4.747634
248.899785	7761.315816	14.385959	-0.052005	4.745252
248.666280	7753.334813	14.390963	-0.051956	4.742885
248.554271	7745.342308	14.395968	-0.051930	4.740512
248.692745	7737.372122	14.400973	-0.051951	4.738145
248.608376	7729.327017	14.405978	-0.051931	4.735754
248.578837	7721.312786	14.410983	-0.051920	4.733371
248.694810	7713.296635	14.415987	-0.051937	4.730986
248.637118	7705.287084	14.420992	-0.051921	4.728603
248.686458	7697.333929	14.425997	-0.051925	4.726234
248.434607	7689.295133	14.431002	-0.051874	4.723840
248.615802	7681.305097	14.436007	-0.051902	4.721458
248.470313	7673.312086	14.441011	-0.051870	4.719075
248.171962	7665.317731	14.446016	-0.051810	4.716690
248.221513	7657.304206	14.451021	-0.051814	4.714298
248.552534	7649.322033	14.456026	-0.051871	4.711913
248.237619	7641.269890	14.461031	-0.051807	4.709507
248.372644	7633.356892	14.466035	-0.051828	4.707141
248.179809	7625.305624	14.471040	-0.051787	4.704733
248.177595	7617.328740	14.476045	-0.051781	4.702346
248.070702	7609.334348	14.481050	-0.051757	4.699952
248.014808	7601.342336	14.486055	-0.051741	4.697558
248.041320	7593.294570	14.491059	-0.051741	4.695146
247.901318	7585.275906	14.496064	-0.051710	4.692741
247.972018	7577.267903	14.501069	-0.051718	4.690338
247.932485	7569.287245	14.506074	-0.051706	4.687942
247.627376	7561.224998	14.511079	-0.051644	4.685521
247.989929	7553.298488	14.516083	-0.051707	4.683138
248.062027	7545.302702	14.521088	-0.051715	4.680734
247.751839	7537.269608	14.526093	-0.051653	4.678318
247.847475	7529.315393	14.531098	-0.051666	4.675924
247.765702	7521.217202	14.536103	-0.051645	4.673485
247.893014	7513.142880	14.541107	-0.051664	4.671052
247.523452	7505.209288	14.546112	-0.051590	4.668661
247.303634	7497.210168	14.551117	-0.051545	4.666249
247.769884	7489.177677	14.556122	-0.051626	4.663824
247.619405	7481.248158	14.561127	-0.051594	4.661430
247.605259	7473.244745	14.566131	-0.051586	4.659012
247.378038	7465.279884	14.571136	-0.051539	4.656605
247.521420	7457.217214	14.576141	-0.051560	4.654167
247.475397	7449.264405	14.581146	-0.051547	4.651761
247.298904	7441.169987	14.586151	-0.051509	4.649311
247.399762	7433.220794	14.591155	-0.051523	4.646903
247.247323	7425.162803	14.596160	-0.051490	4.644461
247.287629	7417.260877	14.601165	-0.051492	4.642066
247.427793	7409.241818	14.606170	-0.051513	4.639633
247.054695	7401.255784	14.611175	-0.051439	4.637209
247.114480	7393.215186	14.616179	-0.051445	4.634768
247.061641	7385.166317	14.621184	-0.051430	4.632322
247.056464	7377.122815	14.626189	-0.051424	4.629877
246.752143	7369.202285	14.631194	-0.051363	4.627468
246.747988	7361.166271	14.636199	-0.051357	4.625023
246.988829	7353.215671	14.641203	-0.051397	4.622602
246.770953	7345.193102	14.646208	-0.051352	4.620158
246.780542	7337.197468	14.651213	-0.051348	4.617721
246.964454	7329.209151	14.656218	-0.051378	4.615285
246.954050	7321.169764	14.661223	-0.051371	4.612832
246.855716	7313.162294	14.666227	-0.051348	4.610387
246.907269	7305.190725	14.671232	-0.051352	4.607952
246.658801	7297.128573	14.676237	-0.051301	4.605489
246.573574	7289.201357	14.681242	-0.051280	4.603065
246.562526	7281.166057	14.686247	-0.051273	4.600606
246.464032	7273.226942	14.691251	-0.051250	4.598176
246.341698	7265.138216	14.696256	-0.051222	4.595699
246.428924	7257.094309	14.701261	-0.051234	4.593234
246.555261	7249.125885	14.706266	-0.051252	4.590791
246.464965	7241.127503	14.711271	-0.051230	4.588337
246.295179	7233.130566	14.716275	-0.051194	4.585883
246.431384	7225.142332	14.721280	-0.051214	4.583430
246.387867	7217.117147	14.726285	-0.051201	4.580964
246.227077	7209.132169	14.731290	-0.051166	4.578509
246.247383	7201.135783	14.736295	-0.051165	4.576050
246.419817	7193.141184	14.741299	-0.051192	4.573590
246.345002	7185.106046	14.746304	-0.051174	4.571116
246.162861	7177.090875	14.751309	-0.051135	4.568646
246.110366	7169.123168	14.756314	-0.051120	4.566190
245.956414	7161.115650	14.761319	-0.051086	4.563720
245.972354	7153.154311	14.766323	-0.051084	4.561263
245.702141	7145.129763	14.771328	-0.051029	4.558786
245.806410	7137.156490	14.776333	-0.051044	4.556323
245.715729	7129.125809	14.781338	-0.051022	4.553840
245.725018	7121.058689	14.786343	-0.051019	4.551345
245.733648	7113.089808	14.791347	-0.051015	4.548880
245.526973	7105.093126	14.796352	-0.050972	4.546404
245.465776	7097.097066	14.801357	-0.050956	4.543927
245.680565	7089.179354	14.806362	-0.050991	4.541473
245.684324	7081.082899	14.811367	-0.050986	4.538962
245.489460	7073.177231	14.816371	-0.050945	4.536509
245.524447	7065.110602	14.821376	-0.050947	4.534005
245.433381	7057.085412	14.826381	-0.050925	4.531512
245.308774	7049.092022	14.831386	-0.050897	4.529028
245.111726	7041.106582	14.836391	-0.050855	4.526544
245.356299	7033.085378	14.841395	-0.050896	4.524049
245.307890	7025.147835	14.846400	-0.050882	4.521578
245.192104	7017.096916	14.851405	-0.050855	4.519070
245.131689	7009.154252	14.856410	-0.050839	4.516594
245.161389	7001.101161	14.861415	-0.050840	4.514083
245.068613	6993.025519	14.866419	-0.050817	4.511564
245.015613	6985.030093	14.871424	-0.050803	4.509068
245.269135	6977.056531	14.876429	-0.050845	4.506578
245.219068	6969.068921	14.881434	-0.050831	4.504081
245.026773	6961.073044	14.886439	-0.050790	4.501581
245.024494	6953.070009	14.891443	-0.050785	4.499077
244.907900	6945.107384	14.896448	-0.050758	4.496584
244.851862	6937.066948	14.901453	-0.050743	4.494065
244.948874	6929.071414	14.906458	-0.050756	4.491560
244.879405	6921.028185	14.911463	-0.050738	4.489038
244.847444	6913.054797	14.916467	-0.050727	4.486536
244.870634	6905.080345	14.921472	-0.050726	4.484033
244.888425	6897.076614	14.926477	-0.050725	4.481519
244.742180	6889.075131	14.931482	-0.050692	4.479004
244.612910	6881.044277	14.936487	-0.050663	4.476478
244.726844	6873.019326	14.941491	-0.050680	4.473954
244.601249	6865.031274	14.946496	-0.050651	4.471439
244.438156	6857.000634	14.951501	-0.050616	4.468909
244.475636	6849.052523	14.956506	-0.050618	4.466404
244.340678	6841.000027	14.961511	-0.050588	4.463864
244.431977	6833.080059	14.966515	-0.050600	4.461366
244.449117	6825.052689	14.971520	-0.050598	4.458831
244.169716	6817.048347	14.976525	-0.050541	4.456302
244.339228	6809.049980	14.981530	-0.050568	4.453775
244.240218	6800.981525	14.986535	-0.050545	4.451223
244.254965	6792.994207	14.991539	-0.050543	4.448696
244.234433	6784.981328	14.996544	-0.050534	4.446159
244.236414	6777.025945	15.001549	-0.050529	4.443639
244.097357	6769.059253	15.006554	-0.050498	4.441113
244.130857	6761.020992	15.011559	-0.050500	4.438564
243.916209	6753.094049	15.016563	-0.050455	4.436047
243.822560	6745.005838	15.021568	-0.050432	4.433479
243.877976	6736.918274	15.026573	-0.050438	4.430910
244.148704	6728.976618	15.031578	-0.050483	4.428387
243.833882	6720.920371	15.036583	-0.050420	4.425823
243.821863	6712.997823	15.041587	-0.050413	4.423302
243.777566	6705.000895	15.046592	-0.050399	4.420755
243.818060	6697.015149	15.051597	-0.050402	4.418211
243.794987	6689.017348	15.056602	-0.050393	4.415661
243.867025	6680.963995	15.061607	-0.050401	4.413093
243.701871	6672.953275	15.066611	-0.050365	4.410535
243.661964	6664.974596	15.071616	-0.050353	4.407987
243.702585	6656.960183	15.076621	-0.050356	4.405426
243.775115	6649.027995	15.081626	-0.050364	4.402891
243.510487	6640.972270	15.086631	-0.050310	4.400312
243.496782	6633.022487	15.091635	-0.050303	4.397767
243.358632	6625.020955	15.096640	-0.050272	4.395204
243.331104	6617.008625	15.101645	-0.050262	4.392636
243.283871	6608.967273	15.106650	-0.050248	4.390057
243.163620	6600.994208	15.111655	-0.050221	4.387498
243.223388	6592.980858	15.116659	-0.050227	4.384926
243.011633	6584.998429	15.121664	-0.050183	4.382361
243.008445	6577.000484	15.126669	-0.050177	4.379790
243.212582	6569.050037	15.131674	-0.050210	4.377235
243.025331	6560.990152	15.136679	-0.050170	4.374640
242.955128	6552.992074	15.141683	-0.050152	4.372064
243.174376	6544.975848	15.146688	-0.050188	4.369483
242.980560	6536.995387	15.151693	-0.050147	4.366909
242.873471	6529.004499	15.156698	-0.050122	4.364331
242.897591	6521.018733	15.161703	-0.050122	4.361754
243.099054	6513.001343	15.166707	-0.050155	4.359166
242.920245	6505.044476	15.171712	-0.050116	4.356594
242.952182	6496.958814	15.176717	-0.050117	4.353980
242.951221	6488.900857	15.181722	-0.050112	4.351373
242.617847	6480.897910	15.186727	-0.050045	4.348780
242.499492	6472.944588	15.191731	-0.050018	4.346203
242.760632	6464.972735	15.196736	-0.050062	4.343621
242.578734	6457.000390	15.201741	-0.050023	4.341035
242.451689	6448.999973	15.206746	-0.049995	4.338438
242.259470	6440.967347	15.211751	-0.049954	4.335828
242.547056	6432.977325	15.216755	-0.050002	4.333235
242.117317	6424.953827	15.221760	-0.049917	4.330623
242.244155	6416.962465	15.226765	-0.049936	4.328025
242.414842	6408.965298	15.231770	-0.049963	4.325423
242.288106	6400.936402	15.236775	-0.049934	4.322808
242.202211	6392.975674	15.241779	-0.049914	4.320213
242.373237	6384.993829	15.246784	-0.049940	4.317612
242.139914	6376.960952	15.251789	-0.049892	4.314989
242.175581	6368.962214	15.256794	-0.049894	4.312378
242.052451	6360.913732	15.261799	-0.049866	4.309748
242.223684	6352.925367	15.266803	-0.049893	4.307139
242.239489	6344.942603	15.271808	-0.049891	4.304528
241.828714	6336.957710	15.276813	-0.049809	4.301912
241.937603	6328.944359	15.281818	-0.049825	4.299289
242.001458	6320.983630	15.286823	-0.049832	4.296681
241.971729	6312.933858	15.291827	-0.049821	4.294042
242.048488	6304.886427	15.296832	-0.049831	4.291402
242.004538	6296.880202	15.301837	-0.049817	4.288774
242.030255	6288.932278	15.306842	-0.049817	4.286164
241.886853	6280.919391	15.311847	-0.049786	4.283529
241.976857	6272.950165	15.316851	-0.049798	4.280909
241.820433	6264.982623	15.321856	-0.049763	4.278286
241.642653	6256.971298	15.326861	-0.049725	4.275646
241.874070	6248.928773	15.331866	-0.049764	4.272999
241.681937	6240.856811	15.336871	-0.049723	4.270336
241.523564	6232.899771	15.341875	-0.049688	4.267710
241.453760	6224.884831	15.346880	-0.049670	4.265063
241.496886	6216.910615	15.351885	-0.049674	4.262430
241.301799	6208.896753	15.356890	-0.049632	4.259780
241.217247	6200.926485	15.361895	-0.049612	4.257143
241.209015	6192.910060	15.366899	-0.049605	4.254490
241.360393	6184.905556	15.371904	-0.049628	4.251841
241.036256	6176.875860	15.376909	-0.049563	4.249178
241.075128	6168.926852	15.381914	-0.049565	4.246543
241.126689	6160.908088	15.386919	-0.049570	4.243883
241.278043	6152.947922	15.391923	-0.049593	4.241243
241.131876	6144.984238	15.396928	-0.049561	4.238596
241.148085	6136.945805	15.401933	-0.049559	4.235925
241.226396	6128.926601	15.406938	-0.049569	4.233258
241.197697	6120.889280	15.411943	-0.049559	4.230583
241.122841	6112.933396	15.416947	-0.049540	4.227933
241.129098	6104.946424	15.421952	-0.049536	4.225272
240.808247	6096.935825	15.426957	-0.049471	4.222598
240.752631	6088.954314	15.431962	-0.049456	4.219935
240.779622	6080.956688	15.436967	-0.049456	4.217265
240.761284	6072.938401	15.441971	-0.049448	4.214587
240.708519	6064.958021	15.446976	-0.049433	4.211919
240.665752	6056.913370	15.451981	-0.049420	4.209227
240.550656	6048.987089	15.456986	-0.049394	4.206573
240.376935	6040.961447	15.461991	-0.049357	4.203884
240.515492	6032.982481	15.466995	-0.049377	4.201211
240.475859	6024.962957	15.472000	-0.049365	4.198522
240.446027	6016.965027	15.477005	-0.049355	4.195838
240.308222	6008.879931	15.482010	-0.049324	4.193122
240.362721	6000.845068	15.487015	-0.049329	4.190423
240.237715	5992.883348	15.492019	-0.049301	4.187745
240.218284	5984.877898	15.497024	-0.049292	4.185051
240.201106	5976.924826	15.502029	-0.049284	4.182374
240.172353	5968.910531	15.507034	-0.049274	4.179674
240.171370	5960.926442	15.512039	-0.049269	4.176983
240.137710	5952.914354	15.517043	-0.049258	4.174280
240.102937	5944.883470	15.522048	-0.049246	4.171569
239.968304	5936.887981	15.527053	-0.049216	4.168867
239.950494	5928.905797	15.532058	-0.049208	4.166170
239.894054	5920.897807	15.537063	-0.049193	4.163461
239.713009	5912.936208	15.542067	-0.049154	4.160765
239.740510	5904.927522	15.547072	-0.049154	4.158053
239.752416	5896.906173	15.552077	-0.049151	4.155336
239.817998	5888.915824	15.557082	-0.049159	4.152627
239.926316	5880.871221	15.562087	-0.049174	4.149899
239.983949	5872.898921	15.567091	-0.049180	4.147193
239.610156	5864.909378	15.572096	-0.049105	4.144475
239.641024	5856.904441	15.577101	-0.049106	4.141754
239.766808	5848.892194	15.582106	-0.049124	4.139030
239.467232	5840.926120	15.587111	-0.049064	4.136315
239.397854	5832.916782	15.592115	-0.049046	4.133586
239.381282	5824.895286	15.597120	-0.049038	4.130852
239.281678	5816.869333	15.602125	-0.049014	4.128113
239.534070	5808.904428	15.607130	-0.049056	4.125398
239.316892	5800.914463	15.612135	-0.049011	4.122666
239.438938	5792.907271	15.617139	-0.049029	4.119932
239.480203	5784.963120	15.622144	-0.049032	4.117215
239.230729	5776.896461	15.627149	-0.048980	4.114452
239.135513	5768.904260	15.632154	-0.048958	4.111714
239.026036	5760.839641	15.637159	-0.048932	4.108949
239.083371	5752.892481	15.642163	-0.048938	4.106225
239.193398	5744.891261	15.647168	-0.048954	4.103481
239.058844	5736.880209	15.652173	-0.048924	4.100728
238.993682	5728.946403	15.657178	-0.048907	4.098002
238.766508	5720.923437	15.662183	-0.048859	4.095240
238.831141	5712.934519	15.667187	-0.048866	4.092493
238.815078	5704.895184	15.672192	-0.048858	4.089725
238.653029	5696.910538	15.677197	-0.048823	4.086972
238.726392	5688.920219	15.682202	-0.048832	4.084218
238.615311	5680.954361	15.687207	-0.048806	4.081468
238.711971	5672.962116	15.692211	-0.048820	4.078711
238.686225	5664.972027	15.697216	-0.048810	4.075950
238.520408	5656.926210	15.702221	-0.048774	4.073167
238.620515	5648.922103	15.707226	-0.048788	4.070399
238.259392	5640.920555	15.712231	-0.048715	4.067625
238.492042	5632.937260	15.717235	-0.048754	4.064863
238.575829	5624.962723	15.722240	-0.048765	4.062100
238.404969	5616.913229	15.727245	-0.048728	4.059305
238.213042	5609.006900	15.732250	-0.048687	4.056558
238.327550	5600.960251	15.737255	-0.048704	4.053765
238.347771	5592.928445	15.742259	-0.048702	4.050973
238.374742	5584.944061	15.747264	-0.048702	4.048197
238.223962	5576.913488	15.752269	-0.048669	4.045399
238.189606	5568.980365	15.757274	-0.048658	4.042636
238.042356	5560.929460	15.762279	-0.048626	4.039827
238.168553	5552.986139	15.767283	-0.048644	4.037059
238.096987	5544.958376	15.772288	-0.048626	4.034256
237.961266	5536.809439	15.777293	-0.048596	4.031408
237.792935	5528.898116	15.782298	-0.048560	4.028640
237.690242	5520.878795	15.787303	-0.048535	4.025834
237.861039	5512.947645	15.792307	-0.048562	4.023060
237.872593	5504.944259	15.797312	-0.048560	4.020258
237.865407	5496.913448	15.802317	-0.048553	4.017443
237.749394	5488.942049	15.807322	-0.048527	4.014645
237.601220	5480.915453	15.812327	-0.048494	4.011826
237.632245	5472.925636	15.817331	-0.048495	4.009020
237.739504	5464.929096	15.822336	-0.048510	4.006211
237.656338	5456.899704	15.827341	-0.048490	4.003386
237.630686	5448.942573	15.832346	-0.048480	4.000585
237.588994	5440.957207	15.837351	-0.048467	3.997771
237.631506	5432.911651	15.842355	-0.048470	3.994936
237.327630	5424.923993	15.847360	-0.048409	3.992114
237.216286	5416.883717	15.852365	-0.048383	3.989274
237.511399	5408.943475	15.857370	-0.048433	3.986474
237.399909	5400.922550	15.862375	-0.048407	3.983637
237.240281	5392.957286	15.867379	-0.048373	3.980817
237.239280	5384.970898	15.872384	-0.048368	3.977990
237.291249	5376.955100	15.877389	-0.048372	3.975152
237.324086	5368.971449	15.882394	-0.048374	3.972322
237.238972	5360.929581	15.887399	-0.048353	3.969468
237.289991	5352.975839	15.892403	-0.048357	3.966646
237.288974	5344.986309	15.897408	-0.048352	3.963807
237.086613	5336.992000	15.902413	-0.048310	3.960962
237.166577	5329.017090	15.907418	-0.048320	3.958126
237.230147	5320.995189	15.912423	-0.048327	3.955271
237.061084	5312.971109	15.917427	-0.048290	3.952410
236.984289	5304.917773	15.922432	-0.048271	3.949537
236.929425	5296.961104	15.927437	-0.048256	3.946698
236.822335	5288.977800	15.932442	-0.048231	3.943845
236.511485	5280.999043	15.937447	-0.048168	3.940989
236.665948	5273.003983	15.942451	-0.048192	3.938133
236.547364	5265.026527	15.947456	-0.048165	3.935276
236.515915	5256.959049	15.952461	-0.048154	3.932387
236.673050	5248.971656	15.957466	-0.048178	3.929527
236.491116	5241.009721	15.962471	-0.048140	3.926669
236.455188	5233.001927	15.967475	-0.048128	3.923795
236.347245	5225.045392	15.972480	-0.048103	3.920935
236.300641	5217.026460	15.977485	-0.048089	3.918052
236.474536	5209.018655	15.982490	-0.048117	3.915175
236.449768	5201.003466	15.987495	-0.048107	3.912290
236.565491	5192.954037	15.992499	-0.048124	3.909393
236.408553	5185.028540	15.997504	-0.048090	3.906533
236.276095	5177.017673	16.002509	-0.048060	3.903641
236.382893	5169.010701	16.007514	-0.048075	3.900752
236.381450	5161.008376	16.012519	-0.048070	3.897861
236.379877	5153.012865	16.017523	-0.048065	3.894971
236.248310	5145.009449	16.022528	-0.048035	3.892072
236.146750	5136.973406	16.027533	-0.048011	3.889161
235.919483	5129.043988	16.032538	-0.047964	3.886283
235.828563	5121.036680	16.037543	-0.047942	3.883378
235.856960	5113.034184	16.042547	-0.047943	3.880475
235.933712	5105.048825	16.047552	-0.047952	3.877576
236.001396	5097.019235	16.052557	-0.047960	3.874659
235.839123	5088.814189	16.057562	-0.047924	3.871672
235.986404	5080.797661	16.062567	-0.047947	3.868757
235.908969	5072.904740	16.067571	-0.047927	3.865880
235.958337	5064.966283	16.072576	-0.047932	3.862987
235.968346	5056.940104	16.077581	-0.047929	3.860059
235.850192	5049.011700	16.082586	-0.047902	3.857163
235.530471	5041.022716	16.087591	-0.047837	3.854237
235.651214	5033.036004	16.092595	-0.047855	3.851319
235.441602	5025.025065	16.097600	-0.047811	3.848384
235.429922	5017.005876	16.102605	-0.047804	3.845447
235.556839	5009.051481	16.107610	-0.047823	3.842534
235.483748	5001.040283	16.112615	-0.047804	3.839595
235.506646	4993.089361	16.117619	-0.047803	3.836677
235.523357	4985.049678	16.122624	-0.047801	3.833724
235.506659	4977.041856	16.127629	-0.047793	3.830780
235.338854	4969.077656	16.132634	-0.047757	3.827847
235.143064	4961.039867	16.137639	-0.047716	3.824883
235.254101	4953.094125	16.142643	-0.047732	3.821958
235.235935	4945.086538	16.147648	-0.047723	3.819005
235.236053	4937.117085	16.152653	-0.047718	3.816064
235.423427	4929.090537	16.157658	-0.047748	3.813104
235.324589	4921.085102	16.162663	-0.047725	3.810143
235.284739	4913.097683	16.167667	-0.047713	3.807187
235.101052	4905.119850	16.172672	-0.047674	3.804230
235.004689	4897.155814	16.177677	-0.047651	3.801278
235.109749	4889.128906	16.182682	-0.047665	3.798304
234.902211	4881.124202	16.187687	-0.047622	3.795329
235.004025	4873.104159	16.192691	-0.047636	3.792353
234.819603	4865.059540	16.197696	-0.047596	3.789360
234.527886	4857.100770	16.202701	-0.047537	3.786393
234.710243	4849.085601	16.207706	-0.047566	3.783414
234.621606	4841.099657	16.212711	-0.047545	3.780437
234.685448	4833.112531	16.217715	-0.047552	3.777461
234.704856	4825.103416	16.222720	-0.047550	3.774473
234.551477	4817.059305	16.227725	-0.047517	3.771466
234.623011	4809.127414	16.232730	-0.047525	3.768504
234.472962	4801.097606	16.237735	-0.047492	3.765497
234.405819	4793.130904	16.242739	-0.047475	3.762514
234.510415	4785.131679	16.247744	-0.047490	3.759520
234.210787	4777.135396	16.252749	-0.047429	3.756515
234.326735	4769.134094	16.257754	-0.047445	3.753516
234.254570	4761.105099	16.262759	-0.047427	3.750499
234.220781	4753.137513	16.267763	-0.047416	3.747504
234.279632	4745.124068	16.272768	-0.047422	3.744492
234.184550	4737.138295	16.277773	-0.047399	3.741484
234.517970	4729.144513	16.282778	-0.047456	3.738481
234.116653	4721.159419	16.287783	-0.047377	3.735461
234.009655	4713.157407	16.292787	-0.047352	3.732439
234.086319	4705.122190	16.297792	-0.047361	3.729406
234.097362	4697.175273	16.302797	-0.047358	3.726403
234.133516	4689.179531	16.307802	-0.047360	3.723380
234.097105	4681.182547	16.312807	-0.047348	3.720352
234.028712	4673.228744	16.317811	-0.047331	3.717337
233.948949	4665.207262	16.322816	-0.047311	3.714294
233.844481	4657.066521	16.327821	-0.047287	3.711202
233.921257	4649.118913	16.332826	-0.047296	3.708186
233.821953	4641.119387	16.337831	-0.047273	3.705143
233.764390	4633.200057	16.342835	-0.047257	3.702129
233.731651	4625.201978	16.347840	-0.047246	3.699083
233.708853	4617.245072	16.352845	-0.047237	3.696050
233.532297	4609.228708	16.357850	-0.047199	3.692989
233.434817	4601.224494	16.362855	-0.047176	3.689932
233.453850	4593.269916	16.367859	-0.047174	3.686893
233.377620	4585.249841	16.372864	-0.047155	3.683825
233.060959	4577.269594	16.377869	-0.047091	3.680764
233.290236	4569.299672	16.382874	-0.047129	3.677718
233.296413	4561.268118	16.387879	-0.047125	3.674640
233.226623	4553.241881	16.392883	-0.047107	3.671559
233.067014	4545.248778	16.397888	-0.047073	3.668487
233.102898	4537.240331	16.402893	-0.047075	3.665411
233.041950	4529.270301	16.407898	-0.047058	3.662344
232.908752	4521.246202	16.412903	-0.047029	3.659253
233.100816	4513.294323	16.417907	-0.047059	3.656195
232.931920	4505.274881	16.422912	-0.047023	3.653098
232.502474	4497.250216	16.427917	-0.046938	3.649991
232.766169	4489.282006	16.432922	-0.046982	3.646921
232.818737	4481.259829	16.437927	-0.046987	3.643821
232.743161	4473.307348	16.442931	-0.046968	3.640743
232.733949	4465.323994	16.447936	-0.046962	3.637652
232.668518	4457.302210	16.452941	-0.046944	3.634542
232.526540	4449.294259	16.457946	-0.046913	3.631432
232.439529	4441.278148	16.462951	-0.046892	3.628318
232.477363	4433.273884	16.467955	-0.046894	3.625210
232.480334	4425.290156	16.472960	-0.046890	3.622106
232.310329	4417.295773	16.477965	-0.046853	3.618990
232.663604	4409.340352	16.482970	-0.046914	3.615901
232.629252	4401.323730	16.487975	-0.046903	3.612775
232.433490	4393.300718	16.492979	-0.046861	3.609639
232.382261	4385.345615	16.497984	-0.046847	3.606531
232.474041	4377.355264	16.502989	-0.046859	3.603411
232.221891	4369.417128	16.507994	-0.046807	3.600298
232.190185	4361.423146	16.512999	-0.046796	3.597168
232.150304	4353.414433	16.518003	-0.046784	3.594028
232.147429	4345.387000	16.523008	-0.046778	3.590880
231.919848	4337.382853	16.528013	-0.046731	3.587731
232.021627	4329.380242	16.533018	-0.046745	3.584590
232.029128	4321.397009	16.538023	-0.046742	3.581451
231.797712	4313.440561	16.543027	-0.046694	3.578312
232.034976	4305.433997	16.548032	-0.046733	3.575165
231.791836	4297.399124	16.553037	-0.046683	3.571990
231.747419	4289.458924	16.558042	-0.046669	3.568855
231.620645	4281.470955	16.563047	-0.046641	3.565696
231.688494	4273.446556	16.568051	-0.046649	3.562526
231.663312	4265.437737	16.573056	-0.046639	3.559356
231.424071	4257.508682	16.578061	-0.046589	3.556209
231.495496	4249.428244	16.583066	-0.046598	3.553008
231.543572	4241.334781	16.588071	-0.046602	3.549798
231.470716	4233.391251	16.593075	-0.046583	3.546642
231.455998	4225.423778	16.598080	-0.046576	3.543474
231.194089	4217.444370	16.603085	-0.046522	3.540292
231.263139	4209.488854	16.608090	-0.046530	3.537126
231.115570	4201.461276	16.613095	-0.046497	3.533923
231.326745	4193.416223	16.618099	-0.046532	3.530720
231.159579	4185.471198	16.623104	-0.046496	3.527542
231.016813	4177.456592	16.628109	-0.046464	3.524335
231.140177	4169.536699	16.633114	-0.046482	3.521171
230.919030	4161.513053	16.638119	-0.046436	3.517952
230.850714	4153.522512	16.643123	-0.046419	3.514748
230.969192	4145.501587	16.648128	-0.046436	3.511534
230.903591	4137.491265	16.653133	-0.046419	3.508316
230.815542	4129.509477	16.658138	-0.046397	3.505106
230.636541	4121.532782	16.663143	-0.046359	3.501893
230.632097	4113.556914	16.668147	-0.046353	3.498682
231.018184	4105.568031	16.673152	-0.046420	3.495475
230.574126	4097.571418	16.678157	-0.046333	3.492236
230.465471	4089.556185	16.683162	-0.046307	3.488997
230.607745	4081.533397	16.688167	-0.046329	3.485759
230.583293	4073.585124	16.693171	-0.046319	3.482544
230.654775	4065.615830	16.698176	-0.046328	3.479320
230.455698	4057.671426	16.703181	-0.046286	3.476095
230.620629	4049.634866	16.708186	-0.046312	3.472841
230.409217	4041.591841	16.713191	-0.046267	3.469569
230.369238	4033.611205	16.718195	-0.046255	3.466325
230.554368	4025.619331	16.723200	-0.046284	3.463081
230.575812	4017.627264	16.728205	-0.046284	3.459828
230.637771	4009.661667	16.733210	-0.046290	3.456584
230.504073	4001.645802	16.738215	-0.046260	3.453310
230.322521	3993.634582	16.743219	-0.046222	3.450034
230.260980	3985.683985	16.748224	-0.046205	3.446783
230.171552	3977.662311	16.753229	-0.046184	3.443499
230.287483	3969.688070	16.758234	-0.046200	3.440238
230.062172	3961.716359	16.763239	-0.046153	3.436963
229.917320	3953.706234	16.768243	-0.046122	3.433673
229.973320	3945.669203	16.773248	-0.046127	3.430375
229.825567	3937.686943	16.778253	-0.046095	3.427089
229.803084	3929.722604	16.783258	-0.046085	3.423812
229.940545	3921.704997	16.788263	-0.046106	3.420515
229.905874	3913.727432	16.793267	-0.046095	3.417226
229.679642	3905.764336	16.798272	-0.046048	3.413933
229.692210	3897.718211	16.803277	-0.046045	3.410610
229.701748	3889.766985	16.808282	-0.046042	3.407324
229.649096	3881.739622	16.813287	-0.046027	3.404000
229.459422	3873.810672	16.818291	-0.045987	3.400710
229.593506	3865.822509	16.823296	-0.046007	3.397403
229.504460	3857.818670	16.828301	-0.045985	3.394078
229.298344	3849.767206	16.833306	-0.045942	3.390726
229.157449	3841.756583	16.838311	-0.045911	3.387390
229.075928	3833.766150	16.843315	-0.045891	3.384062
229.068419	3825.842516	16.848320	-0.045885	3.380760
228.862557	3817.852921	16.853325	-0.045841	3.377421
229.126649	3809.838845	16.858330	-0.045886	3.374085
228.997057	3801.847456	16.863335	-0.045856	3.370741
228.921930	3793.848966	16.868339	-0.045838	3.367392
229.043639	3785.848329	16.873344	-0.045855	3.364047
228.831139	3777.906606	16.878349	-0.045811	3.360711
228.989481	3769.933546	16.883354	-0.045835	3.357371
228.942250	3761.899131	16.888359	-0.045822	3.353996
228.847139	3753.891813	16.893363	-0.045799	3.350626
228.624920	3745.927330	16.898368	-0.045753	3.347266
228.699851	3737.893317	16.903373	-0.045762	3.343885
228.812456	3729.918884	16.908378	-0.045778	3.340527
228.529350	3721.962510	16.913383	-0.045720	3.337158
228.401512	3713.956435	16.918387	-0.045691	3.333771
228.559392	3705.928387	16.923392	-0.045716	3.330381
228.463682	3697.949849	16.928397	-0.045693	3.327000
228.406949	3689.973101	16.933402	-0.045678	3.323617
228.343437	3682.009514	16.938407	-0.045661	3.320236
228.282548	3674.052371	16.943411	-0.045645	3.316855
228.392234	3666.028823	16.948416	-0.045660	3.313448
228.219289	3657.990884	16.953421	-0.045623	3.310021
228.458211	3649.997263	16.958426	-0.045662	3.306625
228.170397	3642.046227	16.963431	-0.045604	3.303223
228.044672	3634.042998	16.968435	-0.045576	3.299802
228.129696	3626.089156	16.973440	-0.045587	3.296407
228.067044	3618.066988	16.978445	-0.045570	3.292973
228.037633	3610.061165	16.983450	-0.045560	3.289544
227.803819	3602.093760	16.988455	-0.045511	3.286119
227.872955	3594.105983	16.993459	-0.045519	3.282695
227.755839	3586.135365	16.998464	-0.045492	3.279266
227.516220	3578.179889	17.003469	-0.045443	3.275836
227.717620	3570.135545	17.008474	-0.045475	3.272381
227.800317	3562.098095	17.013479	-0.045486	3.268921
227.612227	3554.128537	17.018483	-0.045446	3.265476
227.543513	3546.206433	17.023488	-0.045428	3.262053
227.467110	3538.190884	17.028493	-0.045409	3.258585
227.380224	3530.198570	17.033498	-0.045388	3.255123
227.496334	3522.165881	17.038503	-0.045405	3.251648
227.493533	3514.162040	17.043507	-0.045399	3.248177
227.422203	3506.209026	17.048512	-0.045381	3.244721
227.476101	3498.233546	17.053517	-0.045386	3.241257
227.543775	3490.259552	17.058522	-0.045394	3.237791
227.113706	3482.277999	17.063527	-0.045309	3.234297
227.381968	3474.180125	17.068531	-0.045354	3.230778
227.439666	3466.204250	17.073536	-0.045359	3.227299
227.397194	3458.224895	17.078541	-0.045347	3.223811
227.444298	3450.289320	17.083546	-0.045351	3.220341
227.045695	3442.322184	17.088551	-0.045271	3.216836
227.046830	3434.309231	17.093555	-0.045267	3.213324
226.925439	3426.325128	17.098560	-0.045239	3.209815
226.792427	3418.345233	17.103565	-0.045209	3.206304
227.018582	3410.346526	17.108570	-0.045247	3.202795
226.922640	3402.359397	17.113575	-0.045224	3.199274
226.779921	3394.406085	17.118579	-0.045192	3.195763
226.645252	3386.405666	17.123584	-0.045162	3.192227
226.701798	3378.384627	17.128589	-0.045168	3.188686
226.604892	3370.411139	17.133594	-0.045145	3.185155
226.527393	3362.439043	17.138599	-0.045126	3.181623
226.757205	3354.420987	17.143603	-0.045163	3.178079
226.728540	3346.441559	17.148608	-0.045153	3.174537
226.658295	3338.432919	17.153613	-0.045135	3.170976
226.547616	3330.464580	17.158618	-0.045110	3.167427
226.408565	3322.473635	17.163623	-0.045079	3.163864
226.284716	3314.510591	17.168627	-0.045051	3.160309
226.349498	3306.531943	17.173632	-0.045058	3.156751
226.371761	3298.493064	17.178637	-0.045057	3.153161
226.154752	3290.522260	17.183642	-0.045012	3.149587
226.046277	3282.530491	17.188647	-0.044987	3.146004
226.121710	3274.532651	17.193651	-0.044996	3.142422
226.109477	3266.558757	17.198656	-0.044989	3.138843
226.003746	3258.598995	17.203661	-0.044964	3.135262
226.109905	3250.602529	17.208666	-0.044979	3.131670
226.155806	3242.606587	17.213671	-0.044983	3.128071
226.239045	3234.593986	17.218675	-0.044993	3.124462
226.151060	3226.691218	17.223680	-0.044972	3.120891
226.058794	3218.679204	17.228685	-0.044950	3.117267
226.106595	3210.686758	17.233690	-0.044954	3.113653
225.987498	3202.660966	17.238695	-0.044927	3.110012
225.736760	3194.701132	17.243699	-0.044875	3.106391
225.887373	3186.720845	17.248704	-0.044898	3.102775
225.716193	3178.725082	17.253709	-0.044861	3.099133
225.759834	3170.761103	17.258714	-0.044864	3.095511
225.567027	3162.761745	17.263719	-0.044824	3.091858
225.407585	3154.765840	17.268723	-0.044789	3.088203
225.675121	3146.762980	17.273728	-0.044834	3.084560
225.625868	3138.812431	17.278733	-0.044820	3.080923
225.621871	3130.851031	17.283738	-0.044814	3.077278
225.448151	3122.825091	17.288743	-0.044777	3.073592
225.361647	3114.776192	17.293747	-0.044756	3.069895
225.393947	3106.796223	17.298752	-0.044757	3.066230
225.147845	3098.821677	17.303757	-0.044706	3.062550
225.107297	3090.891347	17.308762	-0.044694	3.058896
225.074057	3082.908862	17.313767	-0.044683	3.055214
225.145503	3074.890113	17.318771	-0.044691	3.051516
224.976811	3066.932107	17.323776	-0.044655	3.047830
224.920381	3058.913575	17.328781	-0.044639	3.044116
224.976485	3050.974034	17.333786	-0.044645	3.040441
224.981247	3042.987505	17.338791	-0.044641	3.036736
224.874198	3034.992764	17.343795	-0.044616	3.033018
224.881846	3026.982541	17.348800	-0.044612	3.029293
224.764535	3019.000541	17.353805	-0.044586	3.025571
224.876393	3011.037311	17.358810	-0.044601	3.021864
224.972163	3003.037346	17.363815	-0.044614	3.018135
224.770457	2995.058344	17.368819	-0.044572	3.014397
224.579871	2987.098181	17.373824	-0.044531	3.010663
224.597503	2979.102132	17.378829	-0.044530	3.006918
224.721381	2971.125469	17.383834	-0.044548	3.003182
224.500174	2963.156541	17.388839	-0.044502	2.999428
224.480881	2955.208875	17.393843	-0.044493	2.995690
224.455400	2947.173060	17.398848	-0.044484	2.991905
224.291269	2939.169415	17.403853	-0.044448	2.988124
224.083593	2931.211680	17.408858	-0.044405	2.984357
224.323464	2923.194011	17.413863	-0.044444	2.980580
224.332218	2915.234765	17.418867	-0.044441	2.976814
224.288335	2907.254337	17.423872	-0.044428	2.973030
223.967888	2899.270292	17.428877	-0.044363	2.969226
224.111292	2891.276463	17.433882	-0.044385	2.965436
223.936246	2883.337483	17.438887	-0.044348	2.961651
223.984863	2875.328993	17.443891	-0.044352	2.957839
223.920046	2867.363965	17.448896	-0.044335	2.954038
223.954695	2859.311581	17.453901	-0.044336	2.950194
224.179885	2851.333887	17.458906	-0.044373	2.946392
224.022863	2843.372609	17.463911	-0.044339	2.942572
223.799517	2835.430904	17.468915	-0.044293	2.938754
223.588560	2827.459942	17.473920	-0.044248	2.934917
223.706543	2819.431214	17.478925	-0.044265	2.931064
223.844526	2811.466550	17.483930	-0.044286	2.927239
223.709167	2803.476077	17.488935	-0.044256	2.923381
223.599576	2795.526375	17.493939	-0.044231	2.919540
223.579649	2787.587687	17.498944	-0.044222	2.915703
223.290100	2779.511112	17.503949	-0.044163	2.911780
223.205734	2771.517649	17.508954	-0.044143	2.907903
223.129946	2763.535874	17.513959	-0.044124	2.904027
223.281224	2755.560255	17.518963	-0.044147	2.900161
223.217972	2747.619581	17.523968	-0.044130	2.896296
223.017486	2739.628532	17.528973	-0.044088	2.892393
223.098581	2731.629890	17.533978	-0.044098	2.888496
223.110063	2723.647188	17.538983	-0.044095	2.884598
223.130218	2715.686425	17.543987	-0.044094	2.880706
223.168229	2707.721672	17.548992	-0.044096	2.876808
223.119761	2699.718833	17.553997	-0.044082	2.872882
223.006556	2691.731038	17.559002	-0.044056	2.868953
222.932415	2683.742881	17.564007	-0.044038	2.865021
222.989765	2675.769319	17.569011	-0.044043	2.861098
222.700164	2667.857127	17.574016	-0.043985	2.857181
222.584800	2659.842766	17.579021	-0.043958	2.853218
222.673771	2651.854369	17.584026	-0.043970	2.849273
222.578226	2643.880861	17.589031	-0.043947	2.845320
222.322458	2635.936026	17.594035	-0.043895	2.841367
222.324825	2627.974948	17.599040	-0.043890	2.837414
222.429006	2619.937449	17.604045	-0.043905	2.833424
222.415038	2611.942853	17.609050	-0.043897	2.829443
222.282869	2603.984274	17.614055	-0.043867	2.825467
222.474566	2595.987431	17.619059	-0.043898	2.821486
222.251400	2588.046801	17.624064	-0.043852	2.817502
222.217081	2580.028559	17.629069	-0.043840	2.813486
222.183217	2572.059685	17.634074	-0.043829	2.809488
222.336024	2564.066389	17.639079	-0.043853	2.805483
221.975714	2556.146701	17.644083	-0.043781	2.801480
221.907176	2548.174468	17.649088	-0.043763	2.797461
222.066132	2540.153379	17.654093	-0.043788	2.793425
222.025060	2532.163271	17.659098	-0.043775	2.789388
221.959149	2524.181468	17.664103	-0.043758	2.785347
221.870416	2516.245349	17.669107	-0.043737	2.781322
221.966011	2508.265467	17.674112	-0.043749	2.777280
221.824341	2500.274472	17.679117	-0.043718	2.773212
221.878382	2492.273019	17.684122	-0.043723	2.769145
221.828104	2484.308360	17.689127	-0.043709	2.765084
221.675130	2476.365635	17.694131	-0.043676	2.761022
221.769279	2468.394667	17.699136	-0.043688	2.756955
221.484952	2460.383004	17.704141	-0.043630	2.752838
221.335629	2452.377923	17.709146	-0.043598	2.748726
221.229371	2444.388935	17.714151	-0.043573	2.744619
221.353207	2436.424207	17.719155	-0.043591	2.740533
221.480931	2428.464161	17.724160	-0.043610	2.736442
221.214726	2420.491874	17.729165	-0.043555	2.732316
221.155673	2412.519251	17.734170	-0.043540	2.728195
221.160262	2404.552337	17.739175	-0.043535	2.724076
221.025453	2396.606857	17.744179	-0.043505	2.719952
220.933461	2388.666583	17.749184	-0.043483	2.715828
220.984564	2380.628838	17.754189	-0.043488	2.711655
221.033339	2372.649876	17.759194	-0.043492	2.707507
220.895006	2364.685803	17.764199	-0.043461	2.703348
220.749149	2356.730781	17.769203	-0.043429	2.699187
221.040969	2348.750951	17.774208	-0.043479	2.695034
220.842537	2340.757136	17.779213	-0.043437	2.690836
220.835409	2332.792074	17.784218	-0.043431	2.686659
220.810352	2324.821966	17.789223	-0.043421	2.682472
220.737412	2316.864775	17.794227	-0.043403	2.678282
220.714724	2308.906872	17.799232	-0.043394	2.674088
220.552451	2300.873780	17.804237	-0.043358	2.669839
220.633529	2292.917214	17.809242	-0.043369	2.665640
220.514876	2284.944440	17.814247	-0.043342	2.661412
220.479364	2276.974839	17.819251	-0.043330	2.657184
220.557280	2269.008769	17.824256	-0.043340	2.652959
220.109702	2261.051950	17.829261	-0.043251	2.648698
220.151500	2253.090621	17.834266	-0.043254	2.644460
220.042721	2245.140648	17.839271	-0.043229	2.640211
220.104830	2237.154782	17.844275	-0.043236	2.635947
220.071047	2229.177880	17.849280	-0.043225	2.631674
220.077506	2221.163310	17.854285	-0.043221	2.627378
220.192301	2213.191722	17.859290	-0.043237	2.623104
220.082026	2205.242942	17.864295	-0.043212	2.618821
219.966472	2197.290225	17.869299	-0.043185	2.614528
220.108146	2189.288920	17.874304	-0.043207	2.610219
219.942127	2181.330644	17.879309	-0.043171	2.605906
219.715091	2173.417723	17.884314	-0.043124	2.601606
219.670601	2165.446065	17.889319	-0.043111	2.597279
219.605181	2157.383825	17.894323	-0.043093	2.592894
219.623907	2149.300078	17.899328	-0.043092	2.588496
219.546424	2141.345967	17.904333	-0.043073	2.584155
219.638327	2133.432838	17.909338	-0.043085	2.579840
219.389896	2125.524926	17.914343	-0.043034	2.575497
219.275491	2117.550707	17.919347	-0.043008	2.571120
219.278675	2109.573595	17.924352	-0.043003	2.566742
219.301904	2101.595639	17.929357	-0.043003	2.562358
219.110876	2093.686743	17.934362	-0.042962	2.557989
219.107242	2085.696482	17.939367	-0.042957	2.553581
219.065716	2077.708737	17.944371	-0.042944	2.549164
219.183206	2069.738313	17.949376	-0.042961	2.544759
219.216023	2061.782824	17.954381	-0.042962	2.540350
218.990259	2053.858361	17.959386	-0.042915	2.535932
219.178884	2045.841127	17.964391	-0.042945	2.531484
219.022971	2037.884711	17.969395	-0.042911	2.527037
219.189963	2029.925337	17.974400	-0.042938	2.522604
218.735851	2022.024369	17.979405	-0.042848	2.518152
218.929002	2014.016393	17.984410	-0.042879	2.513678
218.700091	2006.040167	17.989415	-0.042832	2.509183
218.583534	1998.067222	17.994419	-0.042805	2.504691
218.597690	1990.121399	17.999424	-0.042803	2.500215
218.373414	1982.176113	18.004429	-0.042756	2.495713
218.658464	1974.154567	18.009434	-0.042804	2.491198
218.536196	1966.211174	18.014439	-0.042777	2.486689
218.284452	1958.269383	18.019443	-0.042725	2.482163
218.524216	1950.289589	18.024448	-0.042764	2.477644
218.408440	1942.325302	18.029453	-0.042738	2.473099
218.370329	1934.350019	18.034458	-0.042726	2.468545
218.112811	1926.411021	18.039463	-0.042673	2.463987
218.160330	1918.439089	18.044467	-0.042677	2.459424
218.110807	1910.505762	18.049472	-0.042663	2.454868
218.112814	1902.505562	18.054477	-0.042658	2.450268
217.898131	1894.573738	18.059482	-0.042614	2.445683
217.984148	1886.605749	18.064487	-0.042625	2.441092
217.825776	1878.678403	18.069491	-0.042590	2.436496
217.770831	1870.662275	18.074496	-0.042575	2.431849
217.676672	1862.659961	18.079501	-0.042553	2.427197
217.649959	1854.706488	18.084506	-0.042543	2.422570
217.673423	1846.758628	18.089511	-0.042542	2.417941
217.616855	1838.802116	18.094515	-0.042527	2.413293
217.376043	1830.872909	18.099520	-0.042477	2.408636
217.477780	1822.882200	18.104525	-0.042491	2.403962
217.659174	1814.924764	18.109530	-0.042520	2.399304
217.566482	1806.989803	18.114535	-0.042498	2.394629
217.330249	1799.009935	18.119539	-0.042449	2.389907
217.494698	1791.036193	18.124544	-0.042475	2.385210
217.452339	1783.099165	18.129549	-0.042462	2.380510
217.379111	1775.164615	18.134554	-0.042443	2.375800
217.280390	1767.200443	18.139559	-0.042420	2.371060
217.185082	1759.241836	18.144563	-0.042397	2.366315
217.211247	1751.300650	18.149568	-0.042397	2.361580
216.943003	1743.379617	18.154573	-0.042342	2.356824
216.898310	1735.398698	18.159578	-0.042329	2.352040
216.881672	1727.411007	18.164583	-0.042321	2.347245
216.822714	1719.448746	18.169587	-0.042305	2.342452
216.894863	1711.513219	18.174592	-0.042314	2.337676
216.644158	1703.558714	18.179597	-0.042262	2.332852
216.766965	1695.581311	18.184602	-0.042280	2.328035
216.739277	1687.629525	18.189607	-0.042270	2.323212
216.616004	1679.696530	18.194611	-0.042242	2.318381
216.581602	1671.761843	18.199616	-0.042231	2.313547
216.415665	1663.780234	18.204621	-0.042195	2.308663
216.485863	1655.833480	18.209626	-0.042203	2.303810
216.456163	1647.880226	18.214631	-0.042193	2.298934
216.241078	1639.958418	18.219635	-0.042148	2.294052
216.118072	1632.001654	18.224640	-0.042120	2.289145
216.237088	1624.006658	18.229645	-0.042137	2.284225
216.271185	1616.089717	18.234650	-0.042139	2.279335
216.085630	1608.159165	18.239655	-0.042099	2.274407
215.935908	1600.125899	18.244659	-0.042067	2.269408
216.104086	1592.164359	18.249664	-0.042093	2.264470
215.921934	1584.242176	18.254669	-0.042054	2.259515
215.812231	1576.324415	18.259674	-0.042029	2.254559
215.771903	1568.353960	18.264679	-0.042017	2.249565
215.607303	1560.416802	18.269683	-0.041981	2.244569
215.659044	1552.488783	18.274688	-0.041986	2.239587
215.774299	1544.520748	18.279693	-0.042002	2.234574
215.792559	1536.547548	18.284698	-0.042001	2.229539
215.718878	1528.592662	18.289703	-0.041982	2.224495
215.710996	1520.663324	18.294707	-0.041976	2.219462
215.496677	1512.769701	18.299712	-0.041931	2.214421
215.237432	1504.822495	18.304717	-0.041878	2.209331
215.305027	1496.878452	18.309722	-0.041885	2.204261
215.311489	1488.930091	18.314727	-0.041882	2.199170
215.116547	1481.001859	18.319731	-0.041841	2.194063
215.100749	1473.029064	18.324736	-0.041833	2.188931
215.110968	1465.047826	18.329741	-0.041830	2.183784
215.040523	1457.141438	18.334746	-0.041812	2.178666
214.834343	1449.220260	18.339751	-0.041768	2.173513
214.914018	1441.230524	18.344755	-0.041778	2.168330
215.063782	1433.283111	18.349760	-0.041801	2.163169
214.788361	1425.391547	18.354765	-0.041745	2.157993
214.882956	1417.435504	18.359770	-0.041758	2.152796
214.729529	1409.480102	18.364775	-0.041724	2.147564
214.704575	1401.548068	18.369779	-0.041715	2.142346
214.690720	1393.626195	18.374784	-0.041707	2.137124
214.624808	1385.682071	18.379789	-0.041690	2.131869
214.475469	1377.756144	18.384794	-0.041658	2.126605
214.534093	1369.815289	18.389799	-0.041664	2.121338
214.573317	1361.877917	18.394803	-0.041666	2.116058
214.413922	1353.906044	18.399808	-0.041631	2.110723
214.229391	1345.959923	18.404813	-0.041592	2.105390
214.343987	1338.023060	18.409818	-0.041609	2.100077
214.158743	1330.130856	18.414823	-0.041569	2.094753
214.076351	1322.171985	18.419827	-0.041549	2.089379
214.131899	1314.249102	18.424832	-0.041554	2.084030
213.987393	1306.334658	18.429837	-0.041523	2.078653
214.037868	1298.394238	18.434842	-0.041527	2.073264
213.896452	1290.442667	18.439847	-0.041496	2.067834
213.756474	1282.536966	18.444851	-0.041465	2.062421
213.820441	1274.603826	18.449856	-0.041472	2.056995
213.889077	1266.639314	18.454861	-0.041480	2.051534
213.880097	1258.709128	18.459866	-0.041473	2.046074
213.800041	1250.801723	18.464871	-0.041454	2.040609
213.517295	1242.914715	18.469875	-0.041396	2.035122
213.482791	1234.956683	18.474880	-0.041385	2.029596
213.460383	1227.008237	18.479885	-0.041376	2.024062
213.446527	1219.094106	18.484890	-0.041368	2.018539
213.386489	1211.178371	18.489895	-0.041352	2.012994
213.254442	1203.237357	18.494899	-0.041323	2.007409
213.270754	1195.326886	18.499904	-0.041321	2.001846
213.038069	1187.433561	18.504909	-0.041273	1.996252
213.264182	1179.454242	18.509914	-0.041310	1.990631
213.314186	1171.520819	18.514919	-0.041314	1.985007
213.155137	1163.629781	18.519923	-0.041280	1.979376
213.057547	1155.731816	18.524928	-0.041257	1.973730
212.912922	1147.798833	18.529933	-0.041225	1.968037
212.930425	1139.884840	18.534938	-0.041223	1.962360
212.824651	1131.989862	18.539943	-0.041199	1.956666
212.764817	1124.023153	18.544947	-0.041183	1.950908
212.798436	1116.085540	18.549952	-0.041184	1.945165
212.604431	1108.189214	18.554957	-0.041143	1.939410
212.488583	1100.283076	18.559962	-0.041117	1.933639
212.361760	1092.361507	18.564967	-0.041088	1.927838
212.452072	1084.423854	18.569971	-0.041100	1.922032
212.524463	1076.531660	18.574976	-0.041109	1.916240
212.224272	1068.636292	18.579981	-0.041048	1.910387
212.180644	1060.717628	18.584986	-0.041035	1.904527
212.140673	1052.817110	18.589991	-0.041023	1.898662
211.987287	1044.909833	18.594995	-0.040989	1.892762
212.079159	1036.975609	18.600000	-0.041001	1.886851
212.119858	1029.058728	18.605005	-0.041004	1.880928
212.094102	1021.183687	18.610010	-0.040994	1.875011
211.903265	1013.272842	18.615015	-0.040954	1.869028
211.922430	1005.347940	18.620019	-0.040953	1.863040
212.032384	997.434776	18.625024	-0.040968	1.857053
211.745703	989.549373	18.630029	-0.040910	1.851021
211.846221	981.629887	18.635034	-0.040924	1.844988
211.903522	973.737519	18.640039	-0.040930	1.838951
211.746207	965.852451	18.645043	-0.040895	1.832875
211.565954	957.956526	18.650048	-0.040857	1.826767
211.499048	950.064416	18.655053	-0.040840	1.820655
211.373534	942.195419	18.660058	-0.040811	1.814534
211.232399	934.290818	18.665063	-0.040780	1.808362
211.198117	926.396754	18.670067	-0.040769	1.802190
211.232417	918.511742	18.675072	-0.040771	1.796012
211.152470	910.557808	18.680077	-0.040751	1.789745
211.170302	902.654672	18.685082	-0.040749	1.783508
211.094864	894.775131	18.690087	-0.040730	1.777256
211.023775	886.872879	18.695091	-0.040712	1.770965
211.000120	878.996607	18.700096	-0.040703	1.764678
210.780051	871.144000	18.705101	-0.040657	1.758362
210.776685	863.256628	18.710106	-0.040652	1.752023
210.763877	855.349968	18.715111	-0.040644	1.745645
210.837404	847.462497	18.720115	-0.040653	1.739269
210.569132	839.631724	18.725120	-0.040599	1.732872
210.463367	831.738069	18.730125	-0.040574	1.726422
210.379137	823.877622	18.735130	-0.040553	1.719977
210.326786	816.011308	18.740135	-0.040539	1.713507
210.189784	808.104733	18.745139	-0.040508	1.706968
210.367199	800.202827	18.750144	-0.040537	1.700449
210.283427	792.342629	18.755149	-0.040516	1.693905
210.236765	784.460092	18.760154	-0.040503	1.687322
210.061410	776.624401	18.765159	-0.040465	1.680735
209.986592	768.769701	18.770163	-0.040446	1.674120
210.046712	760.872792	18.775168	-0.040453	1.667462
209.759758	753.035438	18.780173	-0.040394	1.660780
209.984627	745.142204	18.785178	-0.040431	1.654092
209.742817	737.296046	18.790183	-0.040382	1.647355
209.707382	729.439275	18.795187	-0.040370	1.640609
209.876456	721.558995	18.800192	-0.040397	1.633843
209.689231	713.660222	18.805197	-0.040357	1.626983
209.607377	705.813342	18.810202	-0.040337	1.620154
209.375576	698.008235	18.815207	-0.040289	1.613312
209.484330	690.108542	18.820211	-0.040304	1.606405
209.346692	682.294066	18.825216	-0.040274	1.599509
209.229038	674.454638	18.830221	-0.040247	1.592563
209.297200	666.584279	18.835226	-0.040255	1.585587
209.305459	658.747757	18.840231	-0.040252	1.578601
209.149823	650.907070	18.845235	-0.040218	1.571556
208.981448	643.097975	18.850240	-0.040182	1.564507
208.803308	635.279403	18.855245	-0.040144	1.557415
208.840331	627.417113	18.860250	-0.040146	1.550283
208.943861	619.554312	18.865255	-0.040160	1.543127
208.874767	611.729625	18.870259	-0.040143	1.535947
208.882338	603.891334	18.875264	-0.040139	1.528733
208.456228	596.114710	18.880269	-0.040055	1.521475
208.500973	588.291691	18.885274	-0.040059	1.514212
208.455911	580.457181	18.890279	-0.040045	1.506888
208.290539	572.651153	18.895283	-0.040010	1.499538
208.344794	564.828118	18.900288	-0.040015	1.492168
208.145694	557.013721	18.905293	-0.039973	1.484731
208.045704	549.236273	18.910298	-0.039950	1.477308
208.086576	541.356108	18.915303	-0.039952	1.469770
208.152744	533.520146	18.920307	-0.039960	1.462240
208.211523	525.718332	18.925312	-0.039966	1.454704
207.896297	517.945787	18.930317	-0.039903	1.447096
207.835738	510.163672	18.935322	-0.039887	1.439480
207.958028	502.352619	18.940327	-0.039905	1.431824
207.887192	494.557922	18.945331	-0.039887	1.424112
207.789856	486.800711	18.950336	-0.039864	1.416391
207.573100	479.027013	18.955341	-0.039818	1.408592
207.529574	471.255268	18.960346	-0.039806	1.400779
207.455117	463.484471	18.965351	-0.039787	1.392919
207.369163	455.686317	18.970355	-0.039766	1.384984
207.209969	447.949126	18.975360	-0.039732	1.377053
207.022768	440.181870	18.980365	-0.039692	1.369041
207.222208	432.383268	18.985370	-0.039724	1.361016
207.008525	424.663249	18.990375	-0.039680	1.352953
206.808739	416.914017	18.995379	-0.039638	1.344813
207.039262	409.119467	19.000384	-0.039676	1.336652
206.875362	401.379133	19.005389	-0.039641	1.328428
206.735463	393.660581	19.010394	-0.039610	1.320181
206.497009	385.903490	19.015399	-0.039561	1.311822
206.426220	378.087817	19.020403	-0.039543	1.303377
206.506559	370.349905	19.025408	-0.039553	1.294989
206.290165	362.648731	19.030413	-0.039508	1.286532
206.411569	354.918648	19.035418	-0.039526	1.278050
206.309432	347.219367	19.040423	-0.039502	1.269504
206.171414	339.520905	19.045427	-0.039472	1.260893
206.175720	331.825563	19.050432	-0.039468	1.252254
205.988545	324.141102	19.055437	-0.039428	1.243531
206.011578	316.447098	19.060442	-0.039428	1.234776
205.811876	308.756230	19.065447	-0.039386	1.225918
205.698554	301.090296	19.070451	-0.039360	1.217042
205.724308	293.401008	19.075456	-0.039360	1.208100
205.632545	285.739629	19.080461	-0.039338	1.199101
205.748411	278.057256	19.085466	-0.039355	1.190052
205.722698	270.398313	19.090471	-0.039345	1.180932
205.452105	262.789201	19.095475	-0.039290	1.171751
205.275562	255.172998	19.100480	-0.039253	1.162508
205.176343	247.534526	19.105485	-0.039230	1.153179
205.219022	239.860385	19.110490	-0.039233	1.143761
205.156784	232.239930	19.115495	-0.039217	1.134309
204.990101	224.636297	19.120499	-0.039181	1.124776
205.228292	217.004987	19.125504	-0.039221	1.115214
204.823366	209.463413	19.130509	-0.039141	1.105543
204.630003	201.907352	19.135514	-0.039100	1.095815
204.666802	194.303728	19.140519	-0.039102	1.085989
204.435608	186.774118	19.145523	-0.039054	1.076110
204.346385	179.206554	19.150528	-0.039033	1.066122
204.206032	171.662268	19.155533	-0.039002	1.056058
204.236519	164.110773	19.160538	-0.039003	1.045928
204.070088	156.606895	19.165543	-0.038968	1.035717
203.830138	149.112820	19.170547	-0.038919	1.025400
204.009691	141.572963	19.175552	-0.038947	1.015016
203.923613	134.079803	19.180557	-0.038927	1.004525
203.793030	126.618490	19.185562	-0.038898	0.993958
203.946978	119.085035	19.190567	-0.038922	0.983244
203.902160	111.633975	19.195571	-0.038909	0.972482
203.530938	104.253441	19.200576	-0.038835	0.961620
203.713014	96.789777	19.205581	-0.038865	0.950653
203.578699	89.403130	19.210586	-0.038835	0.939590
203.291428	82.045620	19.215591	-0.038777	0.928400
202.955209	74.720615	19.220595	-0.038710	0.917109
203.013168	67.332593	19.225600	-0.038716	0.905688
202.742018	60.253287	19.230605	-0.038661	0.894516