Thu Mar 11 18:59:49 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.946521	-0.061021	0.000000	-0.000059	0.724891

0.875151	-0.051699	0.005005	-0.000046	0.724884
0.879560	-0.052038	0.010010	-0.000047	0.724886
0.675788	-0.013121	0.015014	-0.000009	0.724891
0.592114	-0.002885	0.020019	0.000006	0.724883
0.821597	-0.039822	0.025024	-0.000037	0.724891
0.785450	-0.036052	0.030029	-0.000030	0.724886
0.773835	-0.035374	0.035034	-0.000029	0.724884
0.849566	-0.044938	0.040038	-0.000043	0.724892
0.626096	-0.010055	0.045043	-0.000002	0.724883
0.751485	-0.029777	0.050048	-0.000025	0.724888
1.001622	-0.076933	0.055053	-0.000072	0.724884
0.599740	-0.044197	0.060058	0.000003	0.724808
0.778745	-0.184944	0.065062	-0.000031	0.724596
1.006335	-0.230400	0.070067	-0.000073	0.724586
0.984954	-0.221761	0.075072	-0.000070	0.724596
0.680855	-0.169888	0.080077	-0.000013	0.724592
0.572291	-0.151590	0.085082	0.000007	0.724591
0.839197	-0.195630	0.090086	-0.000043	0.724598
0.660243	-0.201329	0.095091	-0.000010	0.724525
0.624697	-0.329988	0.100096	-0.000004	0.724261
0.598825	-0.326650	0.105101	0.000001	0.724259
0.558802	-0.319637	0.110106	0.000008	0.724259
0.653270	-0.334694	0.115110	-0.000010	0.724263
0.538431	-0.318029	0.120115	0.000011	0.724256
0.752501	-0.460156	0.125120	-0.000029	0.724053
0.775096	-0.516889	0.130125	-0.000033	0.723950
0.730122	-0.509871	0.135130	-0.000025	0.723949
0.615061	-0.488980	0.140134	-0.000004	0.723950
0.606424	-0.540822	0.145139	-0.000002	0.723846
0.846868	-0.694000	0.150144	-0.000047	0.723630
0.941029	-0.712988	0.155149	-0.000065	0.723626
0.611694	-0.655222	0.160154	-0.000004	0.723625
0.693544	-0.747639	0.165158	-0.000019	0.723473
0.591909	-0.803272	0.170163	-0.000001	0.723329
0.877795	-0.850941	0.175168	-0.000054	0.723336
0.689560	-0.837803	0.180173	-0.000019	0.723296
0.665493	-0.985268	0.185178	-0.000015	0.722999
0.814622	-1.008232	0.190182	-0.000043	0.723006
0.612126	-0.976429	0.195187	-0.000006	0.722999
0.609949	-1.128246	0.200192	-0.000005	0.722700
0.687991	-1.148896	0.205197	-0.000020	0.722688
0.806173	-1.179200	0.210202	-0.000042	0.722670
0.807879	-1.331560	0.215206	-0.000043	0.722372
0.694805	-1.315873	0.220211	-0.000022	0.722364
0.846048	-1.391495	0.225216	-0.000050	0.722268
0.744199	-1.473117	0.230221	-0.000032	0.722073
0.777093	-1.482822	0.235226	-0.000038	0.722066
0.892638	-1.631730	0.240230	-0.000060	0.721814
0.794424	-1.654198	0.245235	-0.000041	0.721736
0.736115	-1.701362	0.250240	-0.000031	0.721624
0.852212	-1.817137	0.255245	-0.000053	0.721437
0.568044	-1.776614	0.260250	0.000000	0.721418
0.602054	-1.932042	0.265254	-0.000006	0.721125
0.540931	-1.927740	0.270259	0.000005	0.721112
0.662168	-2.040038	0.275264	-0.000018	0.720934
0.372021	-2.019431	0.280269	0.000036	0.720873
0.459369	-2.128758	0.285274	0.000019	0.720689
0.603890	-2.229129	0.290278	-0.000008	0.720543
0.447624	-2.274969	0.295283	0.000021	0.720398
0.255786	-2.328849	0.300288	0.000057	0.720226
0.247523	-2.376401	0.305293	0.000058	0.720129
-0.902289	-2.291262	0.310298	0.000272	0.719894
-4.676703	-1.615354	0.315302	0.000974	0.719902
-3.887653	-1.760069	0.320307	0.000827	0.719894
-4.041020	-1.868015	0.325312	0.000855	0.719628
-5.122902	-1.690582	0.330317	0.001056	0.719599
-5.147727	-1.688729	0.335322	0.001061	0.719594
-5.031212	-1.704009	0.340326	0.001039	0.719605
-5.226385	-1.675264	0.345331	0.001075	0.719594
-5.045058	-1.822805	0.350336	0.001041	0.719367
-5.901697	-1.720863	0.355341	0.001200	0.719268
-6.197958	-1.671143	0.360346	0.001255	0.719262
-5.864604	-1.727102	0.365350	0.001193	0.719269
-6.195767	-1.672868	0.370355	0.001254	0.719261
-6.186449	-1.672266	0.375360	0.001252	0.719265
-6.148272	-1.795564	0.380365	0.001245	0.719036
-6.999463	-1.687680	0.385370	0.001403	0.718950
-7.035206	-1.675969	0.390374	0.001409	0.718961
-7.050052	-1.679016	0.395379	0.001412	0.718951
-6.877242	-1.706861	0.400384	0.001379	0.718957
-6.904689	-1.702719	0.405389	0.001384	0.718956
-7.161222	-1.726370	0.410394	0.001432	0.718819
-8.075316	-1.651242	0.415398	0.001602	0.718647
-7.803816	-1.706196	0.420403	0.001551	0.718634
-8.063541	-1.656295	0.425408	0.001599	0.718642
-7.962632	-1.674855	0.430413	0.001580	0.718641
-8.070341	-1.659423	0.435418	0.001600	0.718634
-8.250268	-1.623774	0.440422	0.001633	0.718642
-8.120161	-1.695616	0.445427	0.001609	0.718546
-8.721147	-1.687285	0.450432	0.001720	0.718352
-8.696017	-1.692625	0.455437	0.001715	0.718351
-9.298582	-1.586919	0.460442	0.001827	0.718348
-8.764435	-1.677227	0.465446	0.001728	0.718358
-8.625839	-1.708113	0.470451	0.001702	0.718346
-9.185240	-1.607763	0.475456	0.001806	0.718348
-8.882958	-1.715942	0.480461	0.001749	0.718241
-9.585932	-1.710062	0.485466	0.001880	0.718006
-9.454699	-1.732878	0.490470	0.001855	0.718007
-9.998868	-1.637451	0.495475	0.001956	0.718005
-9.751976	-1.677273	0.500480	0.001910	0.718014
-9.659758	-1.694878	0.505485	0.001892	0.718012
-9.787054	-1.674887	0.510490	0.001916	0.718007
-9.612321	-1.778532	0.515494	0.001883	0.717864
-10.810155	-1.652141	0.520499	0.002106	0.717693
-10.867783	-1.639502	0.525504	0.002116	0.717698
-10.434571	-1.716067	0.530509	0.002036	0.717699
-10.640602	-1.682998	0.535514	0.002074	0.717693
-10.311278	-1.735648	0.540518	0.002012	0.717705
-10.797098	-1.655706	0.545523	0.002102	0.717693
-10.692622	-1.766031	0.550528	0.002083	0.717512
-11.573292	-1.676230	0.555533	0.002246	0.717380
-11.984334	-1.605931	0.560538	0.002323	0.717374
-11.585213	-1.673860	0.565542	0.002248	0.717381
-11.331166	-1.724120	0.570547	0.002201	0.717371
-11.546280	-1.683825	0.575552	0.002240	0.717376
-11.512130	-1.689430	0.580557	0.002234	0.717377
-11.687762	-1.702227	0.585562	0.002266	0.717291
-12.320588	-1.694071	0.590566	0.002384	0.717084
-12.432046	-1.679736	0.595571	0.002404	0.717074
-12.724130	-1.624825	0.600576	0.002458	0.717080
-12.264616	-1.706552	0.605581	0.002373	0.717081
-12.429527	-1.679816	0.610586	0.002403	0.717076
-12.254412	-1.706388	0.615590	0.002370	0.717085
-12.404120	-1.732226	0.620595	0.002398	0.716982
-13.713611	-1.614372	0.625600	0.002641	0.716754
-13.285682	-1.690672	0.630605	0.002562	0.716754
-13.542453	-1.648282	0.635610	0.002609	0.716748
-13.408717	-1.669615	0.640614	0.002584	0.716754
-13.540932	-1.648425	0.645619	0.002608	0.716749
-13.439073	-1.665303	0.650624	0.002589	0.716752
-13.292777	-1.690884	0.655629	0.002562	0.716754
-13.763856	-1.723399	0.660634	0.002649	0.716524
-14.590382	-1.614440	0.665638	0.002803	0.716448
-14.160096	-1.695222	0.670643	0.002722	0.716441
-14.283220	-1.672340	0.675648	0.002745	0.716443
-14.691695	-1.598942	0.680653	0.002821	0.716445
-14.514604	-1.632691	0.685658	0.002788	0.716441
-14.095107	-1.702643	0.690662	0.002709	0.716451
-14.697348	-1.630558	0.695667	0.002821	0.716382
-15.461929	-1.621439	0.700672	0.002963	0.716130
-15.059312	-1.691697	0.705677	0.002888	0.716134
-15.486813	-1.617825	0.710682	0.002967	0.716130
-15.328494	-1.642753	0.715686	0.002938	0.716137
-15.327186	-1.648734	0.720691	0.002937	0.716126
-15.327644	-1.643959	0.725696	0.002937	0.716135
-15.167892	-1.673477	0.730701	0.002907	0.716134
-15.399043	-1.731370	0.735706	0.002950	0.715938
-16.226049	-1.611654	0.740710	0.003104	0.715884
-16.289951	-1.604599	0.745715	0.003115	0.715876
-15.857748	-1.678397	0.750720	0.003035	0.715882
-15.687174	-1.707045	0.755725	0.003003	0.715886
-16.251574	-1.609887	0.760730	0.003107	0.715880
-16.337898	-1.591078	0.765734	0.003123	0.715887
-16.213296	-1.757310	0.770739	0.003100	0.715602
-17.205144	-1.609707	0.775744	0.003284	0.715545
-17.355346	-1.583300	0.780749	0.003312	0.715545
-17.020768	-1.643923	0.785754	0.003249	0.715543
-16.557587	-1.724738	0.790758	0.003163	0.715547
-16.941808	-1.660028	0.795763	0.003234	0.715540
-17.268175	-1.598971	0.800768	0.003295	0.715546
-17.338031	-1.703259	0.805773	0.003308	0.715315
-18.383258	-1.562263	0.810778	0.003502	0.715226
-18.256903	-1.580205	0.815782	0.003478	0.715236
-18.053279	-1.621473	0.820787	0.003440	0.715226
-18.326219	-1.570052	0.825792	0.003491	0.715232
-17.970264	-1.632162	0.830797	0.003424	0.715235
-18.017290	-1.628305	0.835802	0.003433	0.715227
-17.922614	-1.648433	0.840806	0.003415	0.715221
-18.976920	-1.622162	0.845811	0.003611	0.714901
-19.024133	-1.610050	0.850816	0.003619	0.714908
-18.640125	-1.677907	0.855821	0.003548	0.714910
-18.952089	-1.626338	0.860826	0.003605	0.714903
-19.116755	-1.593538	0.865830	0.003636	0.714910
-18.932009	-1.630419	0.870835	0.003601	0.714902
-18.728574	-1.664534	0.875840	0.003563	0.714907
-19.425921	-1.641276	0.880845	0.003693	0.714707
-20.453256	-1.510141	0.885850	0.003884	0.714605
-19.557423	-1.664585	0.890854	0.003717	0.714615
-19.768239	-1.633352	0.895859	0.003756	0.714603
-20.364186	-1.525644	0.900864	0.003866	0.714607
-19.687651	-1.644832	0.905869	0.003740	0.714610
-19.492516	-1.683249	0.910874	0.003704	0.714603
-20.061735	-1.606089	0.915878	0.003809	0.714555
-20.829020	-1.612241	0.920883	0.003952	0.714272
-20.411658	-1.684944	0.925888	0.003874	0.714276
-20.900216	-1.597349	0.930893	0.003965	0.714277
-21.200655	-1.546845	0.935898	0.004020	0.714272
-20.726983	-1.627145	0.940902	0.003932	0.714280
-21.208779	-1.544055	0.945907	0.004021	0.714275
-20.885341	-1.600378	0.950912	0.003961	0.714279
-20.673923	-1.725729	0.955917	0.003921	0.714105
-22.083395	-1.546607	0.960922	0.004184	0.713962
-21.793295	-1.594008	0.965926	0.004129	0.713971
-21.874634	-1.583558	0.970931	0.004144	0.713964
-21.764688	-1.599804	0.975936	0.004124	0.713971
-21.846971	-1.585691	0.980941	0.004139	0.713970
-22.139488	-1.538049	0.985946	0.004193	0.713962
-21.604030	-1.640082	0.990950	0.004093	0.713949
-22.276231	-1.672542	0.995955	0.004218	0.713647
-22.889949	-1.561193	1.000960	0.004332	0.713651
-22.713586	-1.589863	1.005965	0.004299	0.713657
-22.479462	-1.636323	1.010970	0.004255	0.713648
-22.539080	-1.621223	1.015974	0.004266	0.713658
-22.778526	-1.582797	1.020979	0.004310	0.713650
-22.401649	-1.649549	1.025984	0.004240	0.713651
-23.141139	-1.663752	1.030989	0.004377	0.713361
-23.926594	-1.529062	1.035994	0.004523	0.713351
-23.434269	-1.611087	1.040998	0.004431	0.713363
-23.358664	-1.628792	1.046003	0.004417	0.713355
-23.793619	-1.550782	1.051008	0.004498	0.713356
-23.160246	-1.661862	1.056013	0.004380	0.713360
-23.145793	-1.670633	1.061018	0.004377	0.713348
-24.282690	-1.630003	1.066022	0.004588	0.713027
-24.482526	-1.598826	1.071027	0.004625	0.713018
-24.305706	-1.628013	1.076032	0.004592	0.713023
-23.886803	-1.701119	1.081037	0.004514	0.713027
-24.795576	-1.544293	1.086042	0.004683	0.713017
-24.410312	-1.607248	1.091046	0.004611	0.713029
-24.096125	-1.668206	1.096051	0.004552	0.713020
-25.038826	-1.647433	1.101056	0.004727	0.712727
-25.410300	-1.589944	1.106061	0.004796	0.712710
-25.486066	-1.579538	1.111066	0.004810	0.712705
-25.060025	-1.651722	1.116070	0.004730	0.712712
-25.398536	-1.592972	1.121075	0.004793	0.712710
-25.273205	-1.615692	1.126080	0.004770	0.712709
-25.104330	-1.644838	1.131085	0.004738	0.712712
-25.936171	-1.608636	1.136090	0.004893	0.712489
-26.365756	-1.582247	1.141094	0.004972	0.712390
-25.871127	-1.674061	1.146099	0.004880	0.712383
-26.277594	-1.601280	1.151104	0.004955	0.712384
-26.537139	-1.552876	1.156109	0.005003	0.712389
-26.246958	-1.608614	1.161114	0.004949	0.712381
-26.157100	-1.620195	1.166118	0.004932	0.712391
-26.600601	-1.567928	1.171123	0.005015	0.712338
-26.899208	-1.639247	1.176128	0.005070	0.712090
-26.613346	-1.688497	1.181133	0.005016	0.712094
-27.677821	-1.501052	1.186138	0.005214	0.712090
-27.243982	-1.574437	1.191142	0.005133	0.712098
-26.932445	-1.635899	1.196147	0.005075	0.712087
-27.334275	-1.561984	1.201152	0.005150	0.712092
-27.078868	-1.615912	1.206157	0.005102	0.712076
-27.610721	-1.681168	1.211162	0.005201	0.711757
-27.554789	-1.686317	1.216166	0.005190	0.711767
-28.286747	-1.561210	1.221171	0.005326	0.711757
-28.168486	-1.580284	1.226176	0.005304	0.711761
-27.698055	-1.662659	1.231181	0.005216	0.711765
-28.221981	-1.575913	1.236186	0.005313	0.711752
-27.736151	-1.682915	1.241190	0.005223	0.711712
-28.487237	-1.681238	1.246195	0.005362	0.711449
-28.761103	-1.631221	1.251200	0.005413	0.711452
-28.926902	-1.600383	1.256205	0.005444	0.711455
-28.868690	-1.613140	1.261210	0.005432	0.711450
-28.687756	-1.641701	1.266214	0.005399	0.711458
-29.422938	-1.513862	1.271219	0.005535	0.711452
-29.210417	-1.550556	1.276224	0.005495	0.711455
-29.090749	-1.711383	1.281229	0.005473	0.711177
-30.053094	-1.561208	1.286234	0.005652	0.711135
-30.236361	-1.525732	1.291238	0.005686	0.711141
-29.644925	-1.635659	1.296243	0.005575	0.711133
-29.405368	-1.677524	1.301248	0.005531	0.711135
-29.735401	-1.615777	1.306253	0.005592	0.711141
-29.793823	-1.609431	1.311258	0.005602	0.711133
-29.850436	-1.709966	1.316262	0.005613	0.710913
-30.765861	-1.568649	1.321267	0.005783	0.710870
-30.810220	-1.561367	1.326272	0.005791	0.710869
-30.347602	-1.643101	1.331277	0.005704	0.710871
-30.730778	-1.579742	1.336282	0.005776	0.710862
-30.665719	-1.585899	1.341286	0.005763	0.710873
-30.424683	-1.631156	1.346291	0.005718	0.710869
-31.096763	-1.675703	1.351296	0.005843	0.710541
-31.539981	-1.599569	1.356301	0.005925	0.710536
-31.771408	-1.563483	1.361306	0.005968	0.710526
-31.290707	-1.643323	1.366310	0.005878	0.710538
-31.815028	-1.554299	1.371315	0.005976	0.710530
-31.813702	-1.553908	1.376320	0.005975	0.710532
-31.139622	-1.671842	1.381325	0.005850	0.710536
-31.969927	-1.664987	1.386330	0.006004	0.710255
-32.869647	-1.520738	1.391334	0.006171	0.710223
-32.601109	-1.573553	1.396339	0.006121	0.710214
-32.166030	-1.649133	1.401344	0.006040	0.710218
-32.505848	-1.585565	1.406349	0.006103	0.710225
-32.657550	-1.562941	1.411354	0.006131	0.710216
-32.346419	-1.614285	1.416358	0.006073	0.710225
-32.543377	-1.667950	1.421363	0.006109	0.710048
-34.081331	-1.472224	1.426368	0.006395	0.709892
-33.223553	-1.621264	1.431373	0.006235	0.709900
-33.546750	-1.568426	1.436378	0.006295	0.709891
-33.749450	-1.528084	1.441382	0.006332	0.709900
-33.376759	-1.598366	1.446387	0.006263	0.709893
-33.350815	-1.603378	1.451392	0.006258	0.709892
-33.484314	-1.575524	1.456397	0.006282	0.709901
-33.921449	-1.634462	1.461402	0.006364	0.709628
-33.926459	-1.646796	1.466406	0.006364	0.709602
-34.114484	-1.616757	1.471411	0.006399	0.709595
-34.410282	-1.564585	1.476416	0.006454	0.709595
-34.131484	-1.610797	1.481421	0.006402	0.709602
-34.314717	-1.584071	1.486426	0.006436	0.709591
-34.383350	-1.568209	1.491430	0.006448	0.709598
-34.768394	-1.665153	1.496435	0.006520	0.709268
-34.870795	-1.650879	1.501440	0.006538	0.709260
-35.213901	-1.587271	1.506445	0.006602	0.709266
-35.581912	-1.525543	1.511450	0.006670	0.709258
-35.326828	-1.566673	1.516454	0.006623	0.709267
-35.019914	-1.624881	1.521459	0.006565	0.709261
-35.444324	-1.547914	1.526464	0.006644	0.709264
-35.497746	-1.642316	1.531469	0.006654	0.709056
-36.249421	-1.560318	1.536474	0.006793	0.708953
-36.174039	-1.570281	1.541478	0.006779	0.708960
-36.079527	-1.591257	1.546483	0.006761	0.708952
-36.256897	-1.560150	1.551488	0.006794	0.708952
-36.178790	-1.571223	1.556493	0.006779	0.708958
-36.160833	-1.579958	1.561498	0.006776	0.708947
-36.126293	-1.640062	1.566502	0.006769	0.708840
-37.309829	-1.530565	1.571507	0.006989	0.708637
-37.335032	-1.526539	1.576512	0.006994	0.708637
-37.302690	-1.530197	1.581517	0.006987	0.708641
-37.247077	-1.543537	1.586522	0.006977	0.708635
-37.194896	-1.549212	1.591526	0.006967	0.708643
-37.531784	-1.493843	1.596531	0.007029	0.708634
-37.207991	-1.552875	1.601536	0.006969	0.708632
-37.046761	-1.636937	1.606541	0.006939	0.708521
-38.358065	-1.492035	1.611546	0.007182	0.708344
-37.836785	-1.581555	1.616550	0.007085	0.708351
-37.757201	-1.599321	1.621555	0.007070	0.708344
-38.114333	-1.537536	1.626560	0.007136	0.708341
-37.937870	-1.565676	1.631565	0.007103	0.708348
-38.211892	-1.520651	1.636570	0.007154	0.708341
-38.107345	-1.578269	1.641574	0.007134	0.708263
-39.037245	-1.539890	1.646579	0.007307	0.708009
-38.938473	-1.558000	1.651584	0.007289	0.708008
-38.792794	-1.580383	1.656589	0.007261	0.708016
-39.133252	-1.524721	1.661594	0.007324	0.708006
-38.828258	-1.576940	1.666598	0.007267	0.708011
-38.816404	-1.580570	1.671603	0.007265	0.708008
-39.168331	-1.519126	1.676608	0.007330	0.708006
-39.241553	-1.633740	1.681613	0.007344	0.707751
-39.896059	-1.545991	1.686618	0.007465	0.707693
-39.664635	-1.583660	1.691622	0.007422	0.707701
-39.741528	-1.571237	1.696627	0.007436	0.707699
-39.656381	-1.588475	1.701632	0.007420	0.707695
-39.636216	-1.589188	1.706637	0.007416	0.707701
-39.966795	-1.531587	1.711642	0.007477	0.707699
-40.432734	-1.595514	1.716646	0.007564	0.707405
-40.515526	-1.595652	1.721651	0.007579	0.707375
-40.598306	-1.582529	1.726656	0.007594	0.707372
-40.571438	-1.583972	1.731661	0.007589	0.707380
-40.963842	-1.520717	1.736666	0.007661	0.707367
-40.783486	-1.547807	1.741670	0.007628	0.707377
-40.575332	-1.585647	1.746675	0.007589	0.707376
-41.153279	-1.603683	1.751680	0.007696	0.707134
-41.774400	-1.518200	1.756685	0.007811	0.707083
-42.050339	-1.473640	1.761690	0.007863	0.707075
-41.626798	-1.545324	1.766694	0.007783	0.707083
-41.569227	-1.559356	1.771699	0.007773	0.707076
-41.645280	-1.545410	1.776704	0.007786	0.707077
-41.558257	-1.557072	1.781709	0.007770	0.707085
-41.832950	-1.555301	1.786714	0.007821	0.706991
-42.751110	-1.509317	1.791718	0.007992	0.706755
-42.806852	-1.502100	1.796723	0.008002	0.706750
-42.738615	-1.515312	1.801728	0.007989	0.706748
-42.431218	-1.567114	1.806733	0.007931	0.706755
-42.357366	-1.586494	1.811738	0.007917	0.706743
-42.643277	-1.530555	1.816742	0.007970	0.706753
-42.425682	-1.571284	1.821747	0.007930	0.706750
-43.006768	-1.619562	1.826752	0.008038	0.706445
-43.539844	-1.524614	1.831757	0.008137	0.706446
-43.698609	-1.501129	1.836762	0.008166	0.706436
-43.376353	-1.554300	1.841766	0.008106	0.706445
-43.310465	-1.568957	1.846771	0.008093	0.706440
-43.653073	-1.508428	1.851776	0.008157	0.706439
-43.475784	-1.537933	1.856781	0.008123	0.706444
-43.896067	-1.581725	1.861786	0.008201	0.706206
-44.513836	-1.510852	1.866790	0.008316	0.706127
-44.123225	-1.582112	1.871795	0.008243	0.706125
-44.396530	-1.534906	1.876800	0.008294	0.706122
-44.612375	-1.490800	1.881805	0.008334	0.706134
-44.304935	-1.551310	1.886810	0.008276	0.706123
-44.004907	-1.602308	1.891814	0.008220	0.706128
-44.633952	-1.573358	1.896819	0.008337	0.705962
-45.596137	-1.453838	1.901824	0.008516	0.705857
-44.472261	-1.652050	1.906829	0.008307	0.705862
-44.866381	-1.586915	1.911834	0.008380	0.705852
-45.227926	-1.518932	1.916838	0.008447	0.705860
-45.077498	-1.546175	1.921843	0.008418	0.705860
-45.029264	-1.555316	1.926848	0.008409	0.705859
-45.767340	-1.581451	1.931853	0.008546	0.705542
-46.267856	-1.502891	1.936858	0.008639	0.705521
-46.207638	-1.509592	1.941862	0.008628	0.705530
-46.044168	-1.542069	1.946867	0.008597	0.705523
-46.106727	-1.531420	1.951872	0.008609	0.705523
-46.039424	-1.542293	1.956877	0.008596	0.705526
-46.101884	-1.534106	1.961882	0.008607	0.705520
-46.138102	-1.635226	1.966886	0.008614	0.705304
-46.995789	-1.528734	1.971891	0.008773	0.705211
-46.829340	-1.558988	1.976896	0.008742	0.705210
-46.794877	-1.564162	1.981901	0.008735	0.705213
-47.160301	-1.503437	1.986906	0.008803	0.705204
-46.873699	-1.550614	1.991910	0.008750	0.705213
-47.040626	-1.521437	1.996915	0.008780	0.705212
-47.390580	-1.597062	2.001920	0.008845	0.704935

-47.854458	-1.538807	2.011917	0.008931	0.704886
-47.956779	-1.519944	2.021914	0.008950	0.704889
-47.954362	-1.521576	2.031910	0.008949	0.704887
-47.892046	-1.531558	2.041907	0.008937	0.704890
-47.745346	-1.557904	2.051904	0.008909	0.704891
-47.952297	-1.521008	2.061901	0.008947	0.704892
-47.647440	-1.577101	2.071898	0.008890	0.704889
-47.920891	-1.528117	2.081894	0.008940	0.704891
-47.753756	-1.557562	2.091891	0.008909	0.704892
-47.914675	-1.530425	2.101888	0.008938	0.704890
-48.146761	-1.490949	2.111885	0.008981	0.704887
-47.255745	-1.491104	2.121882	0.008814	0.705208
-46.891035	-1.554334	2.131878	0.008746	0.705212
-47.029006	-1.529465	2.141875	0.008771	0.705214
-47.270492	-1.487383	2.151872	0.008816	0.705213
-46.991775	-1.539786	2.161869	0.008763	0.705208
-46.577377	-1.536791	2.171866	0.008686	0.705364
-46.242338	-1.517610	2.181862	0.008623	0.705523
-46.002287	-1.561528	2.191859	0.008578	0.705522
-46.283721	-1.509219	2.201856	0.008629	0.705527
-46.183915	-1.512833	2.211853	0.008610	0.705557
-45.554084	-1.476093	2.221850	0.008493	0.705858
-45.035516	-1.568727	2.231846	0.008396	0.705858
-45.217581	-1.535881	2.241843	0.008429	0.705860
-45.265705	-1.508998	2.251840	0.008438	0.705898
-44.430224	-1.545185	2.261837	0.008281	0.706125
-44.616069	-1.513570	2.271834	0.008316	0.706123
-44.512917	-1.530828	2.281830	0.008296	0.706126
-43.994518	-1.552443	2.291827	0.008199	0.706270
-43.576194	-1.542398	2.301824	0.008121	0.706441
-43.525435	-1.551521	2.311821	0.008111	0.706441
-43.583689	-1.542301	2.321818	0.008121	0.706440
-42.949840	-1.547273	2.331814	0.008002	0.706658
-42.962273	-1.499497	2.341811	0.008004	0.706750
-42.936273	-1.505296	2.351808	0.007999	0.706749
-42.605756	-1.501056	2.361805	0.007937	0.706877
-41.893829	-1.528942	2.371802	0.007804	0.707076
-41.912104	-1.525565	2.381798	0.007807	0.707078
-41.567157	-1.586776	2.391795	0.007742	0.707079
-41.374002	-1.516124	2.401792	0.007706	0.707291
-40.871199	-1.565712	2.411789	0.007612	0.707372
-41.296971	-1.490868	2.421786	0.007690	0.707371
-40.843505	-1.524141	2.431782	0.007605	0.707467
-40.264370	-1.512914	2.441779	0.007497	0.707698
-40.118648	-1.540092	2.451776	0.007469	0.707697
-40.212957	-1.525227	2.461773	0.007487	0.707694
-39.647133	-1.480874	2.471770	0.007381	0.707986
-39.127717	-1.562692	2.481766	0.007284	0.708008
-39.111856	-1.565515	2.491763	0.007280	0.708009
-39.117695	-1.507711	2.501760	0.007281	0.708124
-38.076884	-1.584036	2.511757	0.007086	0.708344
-38.522702	-1.504963	2.521754	0.007169	0.708344
-38.236582	-1.556969	2.531750	0.007115	0.708343
-37.798572	-1.532566	2.541747	0.007033	0.708549
-37.428539	-1.556496	2.551744	0.006964	0.708634
-37.748360	-1.499490	2.561741	0.007023	0.708635
-37.554614	-1.484737	2.571738	0.006986	0.708735
-36.522404	-1.561764	2.581734	0.006794	0.708950
-36.796866	-1.511790	2.591731	0.006844	0.708953
-36.709332	-1.527933	2.601728	0.006827	0.708953
-36.020162	-1.504306	2.611725	0.006699	0.709247
-35.903348	-1.519068	2.621722	0.006676	0.709260
-35.597110	-1.573524	2.631718	0.006619	0.709261
-35.711236	-1.472841	2.641715	0.006640	0.709423
-34.774668	-1.554508	2.651712	0.006465	0.709594
-35.137445	-1.490553	2.661709	0.006532	0.709594
-34.897528	-1.526038	2.671706	0.006487	0.709609
-34.037156	-1.538872	2.681702	0.006326	0.709891
-34.180869	-1.513060	2.691699	0.006352	0.709892
-33.964192	-1.552490	2.701696	0.006311	0.709892
-33.729296	-1.498762	2.711693	0.006267	0.710084
-33.274575	-1.514921	2.721690	0.006182	0.710214
-33.450028	-1.484548	2.731686	0.006214	0.710213
-33.282062	-1.475836	2.741683	0.006182	0.710291
-32.268346	-1.538933	2.751680	0.005993	0.710527
-32.375067	-1.519048	2.761677	0.006013	0.710530
-32.213911	-1.548231	2.771674	0.005982	0.710530
-31.703543	-1.520958	2.781670	0.005887	0.710767
-31.329666	-1.537790	2.791667	0.005816	0.710867
-31.160066	-1.566989	2.801664	0.005784	0.710870
-31.579763	-1.490901	2.811661	0.005862	0.710874
-30.881886	-1.485585	2.821658	0.005732	0.711133
-30.455650	-1.562512	2.831654	0.005652	0.711132
-30.643958	-1.528637	2.841651	0.005686	0.711134
-29.947465	-1.548288	2.851648	0.005556	0.711343
-29.708398	-1.538623	2.861645	0.005511	0.711449
-29.694950	-1.541640	2.871642	0.005508	0.711448
-29.715766	-1.519706	2.881638	0.005512	0.711486
-29.111418	-1.491799	2.891635	0.005399	0.711757
-28.871453	-1.534474	2.901632	0.005353	0.711758
-29.083199	-1.498226	2.911629	0.005392	0.711756
-28.256749	-1.502938	2.921626	0.005238	0.712041
-28.146315	-1.500415	2.931622	0.005217	0.712086
-27.786795	-1.563685	2.941619	0.005150	0.712089
-27.860784	-1.489471	2.951616	0.005163	0.712211
-26.920390	-1.572885	2.961613	0.004987	0.712380
-27.086234	-1.544269	2.971610	0.005018	0.712379
-27.041186	-1.551465	2.981606	0.005009	0.712381
-26.511388	-1.530536	2.991603	0.004910	0.712612
-26.335698	-1.514461	3.001600	0.004876	0.712707
-26.424504	-1.499454	3.011597	0.004892	0.712707
-25.937865	-1.539758	3.021594	0.004801	0.712800
-25.349664	-1.534973	3.031590	0.004691	0.713019
-25.180626	-1.565476	3.041587	0.004659	0.713019
-25.392575	-1.530061	3.051584	0.004698	0.713015
-24.694872	-1.523105	3.061581	0.004568	0.713278
-24.452093	-1.528639	3.071578	0.004522	0.713354
-24.399331	-1.538779	3.081574	0.004512	0.713353
-24.324230	-1.526064	3.091571	0.004498	0.713406
-23.690751	-1.519967	3.101568	0.004379	0.713643
-23.597686	-1.535951	3.111565	0.004361	0.713645
-23.423096	-1.567206	3.121562	0.004328	0.713646
-23.221821	-1.491650	3.131558	0.004290	0.713868
-22.444665	-1.581582	3.141555	0.004145	0.713966
-22.772654	-1.524200	3.151552	0.004206	0.713965
-22.488654	-1.557369	3.161549	0.004152	0.714000
-21.894837	-1.527889	3.171546	0.004041	0.714270
-21.558481	-1.586350	3.181542	0.003978	0.714274
-21.770113	-1.546670	3.191539	0.004017	0.714279
-21.476445	-1.503289	3.201536	0.003962	0.714470
-20.844838	-1.549057	3.211533	0.003844	0.714603
-20.835545	-1.549995	3.221530	0.003842	0.714605
-20.865068	-1.540831	3.231526	0.003847	0.714614
-20.145640	-1.522222	3.241523	0.003712	0.714906
-20.274310	-1.500274	3.251520	0.003736	0.714905
-20.057975	-1.540539	3.261517	0.003695	0.714903
-19.690778	-1.492166	3.271514	0.003626	0.715130
-19.136483	-1.542055	3.281510	0.003522	0.715227
-19.117774	-1.545182	3.291507	0.003518	0.715229
-19.147415	-1.505734	3.301504	0.003523	0.715297
-18.308380	-1.534372	3.311501	0.003367	0.715538
-18.291769	-1.537716	3.321498	0.003363	0.715538
-18.318910	-1.532281	3.331494	0.003368	0.715540
-17.739438	-1.512899	3.341491	0.003259	0.715784
-17.532121	-1.501439	3.351488	0.003220	0.715881
-17.377228	-1.530363	3.361485	0.003191	0.715879
-17.347695	-1.515857	3.371482	0.003185	0.715919
-16.716761	-1.524232	3.381478	0.003067	0.716126
-16.576999	-1.548566	3.391475	0.003040	0.716128
-16.760052	-1.516264	3.401472	0.003074	0.716129
-16.089717	-1.499146	3.411469	0.002949	0.716400
-15.854437	-1.521275	3.421466	0.002904	0.716440
-15.537140	-1.576167	3.431462	0.002845	0.716444
-15.401960	-1.538901	3.441459	0.002819	0.716567
-14.481976	-1.610977	3.451456	0.002647	0.716749
-14.490186	-1.610689	3.461453	0.002649	0.716748
-14.647175	-1.582518	3.471450	0.002677	0.716749
-14.446045	-1.547294	3.481446	0.002639	0.716891
-13.475255	-1.625055	3.491443	0.002458	0.717080
-13.776269	-1.570953	3.501440	0.002514	0.717082
-13.719677	-1.581813	3.511437	0.002503	0.717081
-13.345034	-1.535931	3.521434	0.002432	0.717305
-12.451683	-1.660624	3.531430	0.002266	0.717374
-12.617018	-1.629228	3.541427	0.002296	0.717379
-12.732262	-1.610587	3.551424	0.002317	0.717376
-12.064749	-1.579459	3.561421	0.002192	0.717673
-11.817346	-1.613116	3.571418	0.002146	0.717695
-11.615199	-1.648715	3.581414	0.002107	0.717697
-11.872543	-1.574279	3.591411	0.002155	0.717754
-10.832145	-1.629101	3.601408	0.001961	0.718013
-10.798377	-1.636885	3.611405	0.001954	0.718010
-10.968107	-1.608146	3.621402	0.001985	0.718008
-10.535234	-1.624113	3.631398	0.001904	0.718130
-10.001033	-1.607816	3.641395	0.001804	0.718351
-9.641931	-1.672318	3.651392	0.001737	0.718351
-10.044455	-1.602078	3.661389	0.001811	0.718349
-9.378356	-1.631366	3.671386	0.001687	0.718526
-8.968725	-1.647935	3.681382	0.001610	0.718638
-9.009454	-1.640828	3.691379	0.001617	0.718639
-8.928862	-1.654022	3.701376	0.001601	0.718642
-8.519393	-1.580607	3.711373	0.001525	0.718932
-8.131027	-1.637998	3.721370	0.001452	0.718956
-7.795087	-1.697303	3.731366	0.001389	0.718958
-8.161157	-1.586378	3.741363	0.001456	0.719049
-7.073760	-1.670231	3.751360	0.001254	0.719267
-7.196001	-1.649717	3.761357	0.001276	0.719265
-6.949024	-1.693928	3.771354	0.001229	0.719265
-6.808212	-1.626128	3.781350	0.001203	0.719450
-6.249557	-1.650203	3.791347	0.001098	0.719599
-6.269144	-1.646782	3.801344	0.001101	0.719600
-6.147990	-1.668267	3.811341	0.001078	0.719601
-5.553393	-1.645261	3.821338	0.000967	0.719856
-5.230903	-1.682530	3.831334	0.000907	0.719897
-5.381939	-1.656453	3.841331	0.000934	0.719896
-5.004688	-1.708273	3.851328	0.000863	0.719927
-4.828625	-1.590429	3.861325	0.000830	0.720222
-4.318969	-1.681813	3.871322	0.000735	0.720221
-4.444444	-1.661519	3.881318	0.000758	0.720218
-4.041815	-1.641959	3.891315	0.000682	0.720399
-3.486546	-1.671116	3.901312	0.000578	0.720537
-3.371450	-1.691599	3.911309	0.000556	0.720538
-3.371403	-1.692310	3.921306	0.000556	0.720538
-2.810700	-1.647633	3.931302	0.000451	0.720823
-2.293546	-1.711271	3.941299	0.000354	0.720880
-2.332307	-1.704594	3.951296	0.000361	0.720880
-2.612789	-1.655786	3.961293	0.000413	0.720879
-1.944505	-1.653599	3.971290	0.000288	0.721118
-1.758239	-1.686715	3.981286	0.000253	0.721119
-1.851965	-1.669892	3.991283	0.000270	0.721120
-1.684419	-1.596858	4.001280	0.000238	0.721324
-1.300411	-1.607425	4.011277	0.000166	0.721438
-1.178427	-1.629888	4.021274	0.000143	0.721438
-1.254855	-1.519885	4.031270	0.000156	0.721628
-0.791683	-1.543208	4.041267	0.000070	0.721745
-0.902206	-1.522003	4.051264	0.000090	0.721749
-0.597953	-1.416838	4.061261	0.000033	0.722063
-0.702181	-1.392893	4.071258	0.000052	0.722074
-0.626789	-1.319309	4.081254	0.000037	0.722246
-0.573460	-1.265701	4.091251	0.000026	0.722371
-0.660053	-1.163835	4.101248	0.000042	0.722542
-0.388893	-1.135326	4.111245	-0.000009	0.722693
-0.493321	-1.013794	4.121242	0.000010	0.722896
-0.110604	-1.027700	4.131238	-0.000062	0.723003
-0.348408	-0.835943	4.141235	-0.000018	0.723297
-0.363888	-0.769233	4.151232	-0.000016	0.723424
-0.235024	-0.686261	4.161229	-0.000040	0.723632
-0.144077	-0.572813	4.171226	-0.000058	0.723887
-0.176160	-0.473128	4.181222	-0.000052	0.724072
0.080919	-0.421787	4.191219	-0.000101	0.724263
0.119011	-0.259644	4.201216	-0.000108	0.724595
-0.074774	-0.121094	4.211213	-0.000073	0.724799
-0.059380	-0.001855	4.221210	-0.000076	0.725039
-0.016071	0.128043	4.231206	-0.000085	0.725309
0.000000	0.315136	4.241203	-0.000089	0.725681

0.020230	0.921163	4.246208	-0.000093	0.726872
0.309859	2.145811	4.251213	-0.000148	0.729358
0.536927	3.966761	4.256218	-0.000192	0.732968
0.440618	6.392952	4.261222	-0.000176	0.737615
1.003349	9.218442	4.266227	-0.000282	0.743219
1.343512	12.568206	4.271232	-0.000348	0.749698
1.597535	16.385552	4.276237	-0.000398	0.756969
2.030395	20.575823	4.281242	-0.000482	0.764921
2.045790	25.241097	4.286246	-0.000488	0.773527
2.425118	30.211516	4.291251	-0.000562	0.782708
2.572664	35.558833	4.296256	-0.000593	0.792384
3.073001	41.162265	4.301261	-0.000690	0.802506
3.393745	47.104477	4.306266	-0.000754	0.813037
3.879033	53.295653	4.311270	-0.000849	0.823912
4.305114	59.785087	4.316275	-0.000933	0.835134
4.580697	66.493040	4.321280	-0.000989	0.846529
5.253265	73.375439	4.326285	-0.001118	0.858176
5.781866	80.491048	4.331290	-0.001222	0.870005
6.161274	87.804115	4.336294	-0.001297	0.881951
6.547127	95.307040	4.341299	-0.001374	0.894040
7.068616	102.926442	4.346304	-0.001477	0.906187
7.813237	110.673173	4.351309	-0.001621	0.918429
8.335621	118.552795	4.356314	-0.001723	0.930654
8.891319	126.539937	4.361318	-0.001832	0.942890
10.592802	134.460404	4.366323	-0.002154	0.955167
11.824896	142.543762	4.371328	-0.002389	0.967406
12.247190	150.875817	4.376333	-0.002474	0.979647
12.974517	159.248348	4.381338	-0.002615	0.991870
14.468658	167.514608	4.386342	-0.002899	1.003983
15.189193	175.982683	4.391347	-0.003039	1.016044
15.775228	184.496823	4.396352	-0.003153	1.027995
16.350340	193.061186	4.401357	-0.003266	1.039874
16.735133	201.680868	4.406362	-0.003344	1.051648
17.144092	210.308808	4.411366	-0.003426	1.063309
17.674007	218.959467	4.416371	-0.003530	1.074900
18.793759	227.483541	4.421376	-0.003745	1.086335
19.537654	236.109479	4.426381	-0.003889	1.097698
20.055833	244.774865	4.431386	-0.003992	1.108944
20.638813	253.422677	4.436390	-0.004106	1.120070
21.749231	261.993745	4.441395	-0.004319	1.131103
22.199190	270.666783	4.446400	-0.004408	1.142015
22.764431	279.346208	4.451405	-0.004519	1.152856
23.341672	287.978716	4.456410	-0.004633	1.163540
23.831277	296.610973	4.461414	-0.004730	1.174109
24.828752	305.149779	4.466419	-0.004921	1.184575
25.623345	313.731504	4.471424	-0.005075	1.194959
26.028674	322.347625	4.476429	-0.005156	1.205215
26.554243	330.954398	4.481434	-0.005260	1.215398
27.533515	339.448960	4.486438	-0.005448	1.225455
28.393711	348.002636	4.491443	-0.005614	1.235474
28.539520	356.596269	4.496448	-0.005647	1.245320
29.417818	365.086611	4.501453	-0.005817	1.255112
30.021896	373.607571	4.506458	-0.005935	1.264810
30.374867	382.159540	4.511462	-0.006006	1.274422
31.217743	390.611150	4.516467	-0.006169	1.283941
31.889287	399.093285	4.521472	-0.006300	1.293392
32.302301	407.596517	4.526477	-0.006383	1.302750
32.715916	416.177753	4.531482	-0.006465	1.312126
32.919862	424.690690	4.536486	-0.006509	1.321323
33.526021	433.092594	4.541491	-0.006628	1.330411
33.855113	441.520505	4.546496	-0.006695	1.339415
34.304375	449.917894	4.551501	-0.006784	1.348347
34.873380	458.300454	4.556506	-0.006896	1.357227
35.213904	466.680802	4.561510	-0.006965	1.366006
35.831438	475.047638	4.566515	-0.007086	1.374763
36.623683	483.354154	4.571520	-0.007239	1.383432
36.973256	491.762389	4.576525	-0.007310	1.392075
37.575549	500.093638	4.581530	-0.007427	1.400630
38.170258	508.412375	4.586534	-0.007544	1.409118
38.766092	516.754081	4.591539	-0.007660	1.417578
38.887460	525.128950	4.596544	-0.007689	1.425944
39.241356	533.489303	4.601549	-0.007760	1.434283
39.829705	541.774591	4.606554	-0.007875	1.442539
40.182966	550.090025	4.611558	-0.007947	1.450739
40.708518	558.404178	4.616563	-0.008050	1.458919
41.231009	566.679968	4.621568	-0.008153	1.467016
41.921855	574.986842	4.626573	-0.008288	1.475124
42.387471	583.263884	4.631578	-0.008380	1.483125
42.792575	591.545598	4.636582	-0.008461	1.491077
43.146267	599.848316	4.641587	-0.008533	1.498998
43.403131	608.130087	4.646592	-0.008586	1.506844
44.117420	616.365512	4.651597	-0.008725	1.514674
44.816155	624.588171	4.656602	-0.008860	1.522451
45.463681	632.818798	4.661606	-0.008987	1.530187
45.936300	641.089845	4.666611	-0.009080	1.537894
46.363549	649.339538	4.671616	-0.009165	1.545537
46.894397	657.607542	4.676621	-0.009270	1.553175
47.403762	665.831839	4.681626	-0.009370	1.560731
47.927979	674.043802	4.686630	-0.009473	1.568243
48.466335	682.289024	4.691635	-0.009579	1.575750
48.657297	690.548245	4.696640	-0.009620	1.583184
49.039253	698.787427	4.701645	-0.009697	1.590592
49.510773	707.014139	4.706650	-0.009791	1.597968
49.844271	715.219884	4.711654	-0.009858	1.605272
50.019138	723.499544	4.716659	-0.009897	1.612585
50.302521	731.708609	4.721664	-0.009955	1.619818
50.846097	739.891954	4.726669	-0.010062	1.627033
51.370987	748.152019	4.731674	-0.010165	1.634280
51.801518	756.311741	4.736678	-0.010251	1.641395
52.256564	764.502214	4.741683	-0.010341	1.648509
52.912185	772.655262	4.746688	-0.010469	1.655587
53.514275	780.812521	4.751693	-0.010586	1.662632
54.059261	788.999051	4.756698	-0.010693	1.669663
54.426819	797.194710	4.761702	-0.010767	1.676649
54.924025	805.379774	4.766707	-0.010866	1.683614
55.118986	813.598665	4.771712	-0.010907	1.690539
55.615367	821.779747	4.776717	-0.011005	1.697444
56.083816	829.954772	4.781722	-0.011098	1.704311
56.268269	838.168822	4.786726	-0.011138	1.711146
57.080249	846.300896	4.791731	-0.011295	1.717968
57.311819	854.490856	4.796736	-0.011344	1.724735
57.614889	862.683330	4.801741	-0.011406	1.731487
58.036369	870.860437	4.806746	-0.011490	1.738215
58.312985	879.008121	4.811750	-0.011547	1.744875
58.529010	887.224920	4.816755	-0.011593	1.751557
58.812470	895.393233	4.821760	-0.011651	1.758184
59.224296	903.514482	4.826765	-0.011733	1.764763
59.588397	911.685440	4.831770	-0.011807	1.771352
59.808591	919.847081	4.836774	-0.011853	1.777892
60.240672	927.987797	4.841779	-0.011939	1.784416
61.172313	936.077080	4.846784	-0.012118	1.790938
61.580507	944.261079	4.851789	-0.012200	1.797446
62.167610	952.362543	4.856794	-0.012314	1.803887
62.785821	960.479568	4.861798	-0.012435	1.810322
63.034929	968.669867	4.866803	-0.012487	1.816746
63.224662	976.825813	4.871808	-0.012528	1.823113
63.687477	984.957934	4.876813	-0.012620	1.829472
64.307442	993.092417	4.881818	-0.012741	1.835830
64.424573	1001.249879	4.886822	-0.012768	1.842124
65.085141	1009.363007	4.891827	-0.012897	1.848426
65.194973	1017.547543	4.896832	-0.012923	1.854697
65.546153	1025.675575	4.901837	-0.012994	1.860931
65.965177	1033.811581	4.906842	-0.013077	1.867159
66.154602	1041.988103	4.911846	-0.013118	1.873370
66.568765	1050.111276	4.916851	-0.013201	1.879546
66.972889	1058.193230	4.921856	-0.013281	1.885669
67.421567	1066.322397	4.926861	-0.013370	1.891813
67.828693	1074.465475	4.931866	-0.013452	1.897943
68.152318	1082.572761	4.936870	-0.013518	1.904017
68.509627	1090.721578	4.941875	-0.013590	1.910105
68.821617	1098.854147	4.946880	-0.013653	1.916158
68.951945	1106.987600	4.951885	-0.013683	1.922171
69.321109	1115.104467	4.956890	-0.013757	1.928180
69.460636	1123.253656	4.961894	-0.013789	1.934169
69.750574	1131.375020	4.966899	-0.013848	1.940135
70.022446	1139.485528	4.971904	-0.013905	1.946073
70.647658	1147.604635	4.976909	-0.014027	1.952038
71.260259	1155.707840	4.981914	-0.014146	1.957971
71.246991	1163.830868	4.986918	-0.014149	1.963833
71.780481	1171.909267	4.991923	-0.014254	1.969705
72.071317	1180.022976	4.996928	-0.014314	1.975558
72.245485	1188.140165	5.001933	-0.014352	1.981383
72.619225	1196.244685	5.006938	-0.014427	1.987204
72.929191	1204.356847	5.011942	-0.014490	1.993006
73.574360	1212.425296	5.016947	-0.014616	1.998796
73.807670	1220.525932	5.021952	-0.014665	2.004548
73.948846	1228.662587	5.026957	-0.014696	2.010300
74.394384	1236.772106	5.031962	-0.014785	2.016047
74.638352	1244.866692	5.036966	-0.014836	2.021747
75.148868	1252.961346	5.041971	-0.014936	2.027458
75.145062	1261.148750	5.046976	-0.014941	2.033165
75.644977	1269.209059	5.051981	-0.015040	2.038819
76.003605	1277.282254	5.056986	-0.015112	2.044452
76.461212	1285.362369	5.061990	-0.015203	2.050084
76.709084	1293.484938	5.066995	-0.015255	2.055709
76.967608	1301.580436	5.072000	-0.015308	2.061300
78.125689	1309.555057	5.077005	-0.015529	2.066884
78.850238	1317.659340	5.082010	-0.015670	2.072498
79.031127	1325.789547	5.087014	-0.015709	2.078060
79.097831	1333.932805	5.092019	-0.015727	2.083605
79.397323	1342.037719	5.097024	-0.015788	2.089131
79.657230	1350.166860	5.102029	-0.015842	2.094656
79.979715	1358.255560	5.107034	-0.015908	2.100145
80.101657	1366.363594	5.112038	-0.015936	2.105613
80.797493	1374.452706	5.117043	-0.016071	2.111110
81.028745	1382.593166	5.122048	-0.016120	2.116582
81.085946	1390.680022	5.127053	-0.016136	2.121987
81.527214	1398.742825	5.132058	-0.016224	2.127399
81.789606	1406.829878	5.137062	-0.016278	2.132796
82.119406	1414.924653	5.142067	-0.016345	2.138191
82.518491	1422.984566	5.147072	-0.016425	2.143556
82.913037	1431.059475	5.152077	-0.016504	2.148917
83.159379	1439.200058	5.157082	-0.016555	2.154294
83.379980	1447.258593	5.162086	-0.016602	2.159601
83.817376	1455.325325	5.167091	-0.016689	2.164921
84.004264	1463.429476	5.172096	-0.016729	2.170228
84.492688	1471.492501	5.177101	-0.016825	2.175524
84.985750	1479.547704	5.182106	-0.016923	2.180802
85.057778	1487.655495	5.187110	-0.016942	2.186063
85.268969	1495.780827	5.192115	-0.016986	2.191335
85.571761	1503.863747	5.197120	-0.017048	2.196575
85.962962	1511.917524	5.202125	-0.017127	2.201792
86.200166	1520.002438	5.207130	-0.017176	2.207002
86.380940	1528.090430	5.212134	-0.017215	2.212198
86.594748	1536.194158	5.217139	-0.017261	2.217394
87.045531	1544.227382	5.222144	-0.017350	2.222554
87.264002	1552.322026	5.227149	-0.017396	2.227720
87.566237	1560.423409	5.232154	-0.017458	2.232886
87.997620	1568.465966	5.237158	-0.017544	2.238014
88.485528	1576.508012	5.242163	-0.017640	2.243135
88.770026	1584.611803	5.247168	-0.017699	2.248265
88.817526	1592.727045	5.252173	-0.017713	2.253370
89.316523	1600.796705	5.257178	-0.017812	2.258474
89.503356	1608.852909	5.262182	-0.017852	2.263531
90.124539	1616.901337	5.267187	-0.017973	2.268610
90.401680	1625.067326	5.272192	-0.018030	2.273720
90.447062	1633.141872	5.277197	-0.018044	2.278743
90.890941	1641.175471	5.282202	-0.018132	2.283762
91.036295	1649.229842	5.287206	-0.018165	2.288759
91.210566	1657.342240	5.292211	-0.018203	2.293782
91.484790	1665.390831	5.297216	-0.018259	2.298764
91.686702	1673.448454	5.302221	-0.018302	2.303734
92.195635	1681.497587	5.307226	-0.018403	2.308714
92.350798	1689.603196	5.312230	-0.018437	2.313688
92.769721	1697.644763	5.317235	-0.018521	2.318634
93.068792	1705.699652	5.322240	-0.018582	2.323568
93.145742	1713.791365	5.327245	-0.018602	2.328496
93.388868	1721.890796	5.332250	-0.018652	2.333431
93.852146	1729.924469	5.337254	-0.018744	2.338334
94.147734	1737.993954	5.342259	-0.018805	2.343234
94.315573	1746.076352	5.347264	-0.018841	2.348122
94.536406	1754.181008	5.352269	-0.018888	2.353017
95.006688	1762.230739	5.357274	-0.018981	2.357889
95.112450	1770.277802	5.362278	-0.019006	2.362720
95.603462	1778.329219	5.367283	-0.019103	2.367575
95.957768	1786.396522	5.372288	-0.019175	2.372418
96.146903	1794.476254	5.377293	-0.019215	2.377246
96.548287	1802.519357	5.382298	-0.019296	2.382058
96.880991	1810.564498	5.387302	-0.019363	2.386857
97.148343	1818.671760	5.392307	-0.019418	2.391678
97.512712	1826.708284	5.397312	-0.019492	2.396454
97.730821	1834.773448	5.402317	-0.019538	2.401227
97.999377	1842.852608	5.407322	-0.019593	2.406002
98.034898	1850.936160	5.412326	-0.019606	2.410752
98.419047	1859.006189	5.417331	-0.019683	2.415512
98.846730	1867.033735	5.422336	-0.019768	2.420241
99.253426	1875.080586	5.427341	-0.019849	2.424970
99.446594	1883.175675	5.432346	-0.019890	2.429701
99.774414	1891.308404	5.437350	-0.019957	2.434456
99.897138	1899.363141	5.442355	-0.019985	2.439140
100.046847	1907.404544	5.447360	-0.020019	2.443810
100.257002	1915.451599	5.452365	-0.020063	2.448478
100.590613	1923.510955	5.457370	-0.020131	2.453154
100.720219	1931.562456	5.462374	-0.020160	2.457801
101.045953	1939.608249	5.467379	-0.020227	2.462451
101.386192	1947.652596	5.472384	-0.020295	2.467092
101.632102	1955.716439	5.477389	-0.020347	2.471729
102.074032	1963.771425	5.482394	-0.020435	2.476366
102.446358	1971.795261	5.487398	-0.020509	2.480971
102.729777	1979.853482	5.492403	-0.020568	2.485581
102.900224	1987.928032	5.497408	-0.020605	2.490184
103.507768	1995.971512	5.502413	-0.020723	2.494792
103.960894	2004.027598	5.507418	-0.020813	2.499387
104.040556	2012.089520	5.512422	-0.020834	2.503950
104.114568	2020.197396	5.517427	-0.020853	2.508530
104.347597	2028.299962	5.522432	-0.020902	2.513111
104.742422	2036.313855	5.527437	-0.020981	2.517645
104.832316	2044.386583	5.532442	-0.021003	2.522181
104.890291	2052.428072	5.537446	-0.021019	2.526690
105.139238	2060.496150	5.542451	-0.021071	2.531219
105.423422	2068.553068	5.547456	-0.021130	2.535736
105.627954	2076.597399	5.552461	-0.021173	2.540233
105.983940	2084.644983	5.557466	-0.021245	2.544734
106.220932	2092.692904	5.562470	-0.021295	2.549218
106.519489	2100.771303	5.567475	-0.021356	2.553716
106.959036	2108.799953	5.572480	-0.021443	2.558189
107.172155	2116.838484	5.577485	-0.021488	2.562643
107.545005	2124.892216	5.582490	-0.021563	2.567109
107.672350	2132.964493	5.587494	-0.021592	2.571560
107.962262	2141.038900	5.592499	-0.021652	2.576016
108.162185	2149.075262	5.597504	-0.021694	2.580437
108.544024	2157.083289	5.602509	-0.021771	2.584847
108.971720	2165.155516	5.607514	-0.021856	2.589288
109.059832	2173.396919	5.612518	-0.021878	2.593791
109.319329	2181.422167	5.617523	-0.021932	2.598179
110.013463	2189.366975	5.622528	-0.022067	2.602546
110.224344	2197.386334	5.627533	-0.022111	2.606914
110.582476	2205.442188	5.632538	-0.022184	2.611303
110.967470	2213.469499	5.637542	-0.022261	2.615672
111.221619	2221.510783	5.642547	-0.022314	2.620031
111.506299	2229.530548	5.647552	-0.022372	2.624374
111.895006	2237.582265	5.652557	-0.022450	2.628734
111.923603	2245.697847	5.657562	-0.022461	2.633097
112.184539	2253.719953	5.662566	-0.022515	2.637418
112.520300	2261.752590	5.667571	-0.022583	2.641743
112.843592	2269.792241	5.672576	-0.022648	2.646063
112.930505	2277.852271	5.677581	-0.022670	2.650372
113.122273	2285.954262	5.682586	-0.022711	2.654702
113.706779	2293.936748	5.687590	-0.022826	2.658988
113.968383	2301.977753	5.692595	-0.022880	2.663276
114.312873	2310.038868	5.697600	-0.022950	2.667574
114.498907	2318.110049	5.702605	-0.022990	2.671860
114.822446	2326.184109	5.707610	-0.023055	2.676149
115.170308	2334.194968	5.712614	-0.023126	2.680400
115.469278	2342.211630	5.717619	-0.023187	2.684644
115.679665	2350.270870	5.722624	-0.023231	2.688898
115.857871	2358.351645	5.727629	-0.023270	2.693154
116.110158	2366.401244	5.732634	-0.023323	2.697392
116.198878	2374.438580	5.737638	-0.023345	2.701606
116.628449	2382.461938	5.742643	-0.023430	2.705828
116.874408	2390.526682	5.747648	-0.023481	2.710053
117.205793	2398.563365	5.752653	-0.023549	2.714263
117.566180	2406.626070	5.757658	-0.023621	2.718481
117.594935	2414.651480	5.762662	-0.023632	2.722652
117.813777	2422.712956	5.767667	-0.023678	2.726848
118.004187	2430.783730	5.772672	-0.023719	2.731040
118.308915	2438.824452	5.777677	-0.023781	2.735217
118.481781	2446.877547	5.782682	-0.023819	2.739387
118.663600	2454.903177	5.787686	-0.023858	2.743536
118.969265	2462.948892	5.792691	-0.023921	2.747696
119.193612	2471.043321	5.797696	-0.023968	2.751871
119.428564	2479.146494	5.802701	-0.024017	2.756044
119.808805	2487.146857	5.807706	-0.024094	2.760167
119.928299	2495.134443	5.812710	-0.024121	2.764261
120.012177	2503.189484	5.817715	-0.024142	2.768382
120.342897	2511.232611	5.822720	-0.024209	2.772505
120.685888	2519.265622	5.827725	-0.024279	2.776618
120.868543	2527.314079	5.832730	-0.024318	2.780723
120.936998	2535.336775	5.837734	-0.024337	2.784802
121.491582	2543.354227	5.842739	-0.024445	2.788901
121.943817	2551.417875	5.847744	-0.024535	2.793011
122.170193	2559.448763	5.852749	-0.024583	2.797085
122.442221	2567.494261	5.857754	-0.024639	2.801163
122.628411	2575.520653	5.862758	-0.024679	2.805221
122.893168	2583.570206	5.867763	-0.024734	2.809289
123.159306	2591.637018	5.872768	-0.024789	2.813360
123.447419	2599.660245	5.877773	-0.024848	2.817404
123.647906	2607.730144	5.882778	-0.024891	2.821461
123.810971	2615.761756	5.887782	-0.024927	2.825490
124.318919	2623.794914	5.892787	-0.025027	2.829534
124.391834	2631.905740	5.897792	-0.025046	2.833587
124.626127	2639.908930	5.902797	-0.025095	2.837589
124.974191	2647.933225	5.907802	-0.025165	2.841602
125.233925	2655.950796	5.912806	-0.025219	2.845601
125.545121	2663.992226	5.917811	-0.025282	2.849610
125.848693	2672.063672	5.922816	-0.025344	2.853627
126.156881	2680.081122	5.927821	-0.025407	2.857612
126.426947	2688.136993	5.932826	-0.025463	2.861608
126.176213	2696.197651	5.937830	-0.025422	2.865572
126.513414	2704.222982	5.942835	-0.025490	2.869546
126.831460	2712.279552	5.947840	-0.025555	2.873528
126.861610	2720.329472	5.952845	-0.025566	2.877486
127.168846	2728.345545	5.957850	-0.025629	2.881437
127.451817	2736.344902	5.962854	-0.025687	2.885373
127.659157	2744.410360	5.967859	-0.025731	2.889331
127.894443	2752.462802	5.972864	-0.025780	2.893280
128.138547	2760.503638	5.977869	-0.025831	2.897218
128.575174	2768.539366	5.982874	-0.025918	2.901158
128.740153	2776.552102	5.987878	-0.025954	2.905067
129.168163	2784.605838	5.992883	-0.026039	2.909005
129.471319	2792.721162	5.997888	-0.026101	2.912960
129.646706	2800.757976	6.002893	-0.026139	2.916866
130.079219	2808.778737	6.007898	-0.026225	2.920771
130.438907	2816.738323	6.012902	-0.026298	2.924639
130.525653	2824.808374	6.017907	-0.026319	2.928540
130.648929	2832.879421	6.022912	-0.026348	2.932438
130.909915	2840.906052	6.027917	-0.026402	2.936317
131.504838	2848.902575	6.032922	-0.026518	2.940193
131.630459	2856.940114	6.037926	-0.026547	2.944060
131.848442	2864.973724	6.042931	-0.026593	2.947924
132.062707	2873.047753	6.047936	-0.026638	2.951803
132.178074	2881.110549	6.052941	-0.026665	2.955665
132.262317	2889.117345	6.057946	-0.026687	2.959495
132.454256	2897.140655	6.062950	-0.026728	2.963333
132.752173	2905.169651	6.067955	-0.026789	2.967174
132.859571	2913.237519	6.072960	-0.026814	2.971019
132.941984	2921.273220	6.077965	-0.026835	2.974842
133.265586	2929.295521	6.082970	-0.026901	2.978666
133.572218	2937.312325	6.087974	-0.026963	2.982482
133.886058	2945.357936	6.092979	-0.027027	2.986306
134.156498	2953.374375	6.097984	-0.027083	2.990110
134.407016	2961.468782	6.102989	-0.027135	2.993945
134.798636	2969.485243	6.107994	-0.027214	2.997745
135.018399	2977.504377	6.112998	-0.027260	3.001533
135.286378	2985.516725	6.118003	-0.027315	3.005315
135.299848	2993.582727	6.123008	-0.027323	3.009105
135.399487	3001.621897	6.128013	-0.027347	3.012882
135.915625	3009.654204	6.133018	-0.027449	3.016672
135.956698	3017.685874	6.138022	-0.027462	3.020433
136.151023	3025.700879	6.143027	-0.027504	3.024189
136.520577	3033.745826	6.148032	-0.027578	3.027963
136.678045	3041.800976	6.153037	-0.027613	3.031727
136.810360	3049.894329	6.158042	-0.027643	3.035502
137.120094	3057.859212	6.163046	-0.027706	3.039222
137.525470	3065.875229	6.168051	-0.027787	3.042965
137.741070	3073.942485	6.173056	-0.027833	3.046718
137.918367	3081.968478	6.178061	-0.027871	3.050446
138.144006	3090.037886	6.183066	-0.027919	3.054191
138.233796	3098.061671	6.188070	-0.027941	3.057905
138.437556	3106.094404	6.193075	-0.027984	3.061623
138.997688	3114.091063	6.198080	-0.028094	3.065337
139.160453	3122.111170	6.203085	-0.028130	3.069038
139.183555	3130.265982	6.208090	-0.028140	3.072791
139.480651	3138.290036	6.213094	-0.028201	3.076491
139.803860	3146.259990	6.218099	-0.028266	3.080163
139.970916	3154.277947	6.223104	-0.028303	3.083846
140.432913	3162.269605	6.228109	-0.028394	3.087526
140.865202	3170.321181	6.233114	-0.028480	3.091228
140.918861	3178.375645	6.238118	-0.028496	3.094908
141.267164	3186.406675	6.243123	-0.028566	3.098588
141.335506	3194.454282	6.248128	-0.028584	3.102257
141.620519	3202.457489	6.253133	-0.028643	3.105912
141.864575	3210.523169	6.258138	-0.028694	3.109589
141.778889	3218.599092	6.263142	-0.028683	3.113252
142.023878	3226.600575	6.268147	-0.028734	3.116891
142.332831	3234.638980	6.273152	-0.028797	3.120546
142.464198	3242.617582	6.278157	-0.028827	3.124161
142.634303	3250.677712	6.283162	-0.028864	3.127811
142.999645	3258.716983	6.288166	-0.028938	3.131455
143.203330	3266.763738	6.293171	-0.028981	3.135092
143.563053	3274.795569	6.298176	-0.029054	3.138724
143.747842	3282.795733	6.303181	-0.029094	3.142330
143.829245	3290.857742	6.308186	-0.029114	3.145956
144.047392	3298.874645	6.313190	-0.029160	3.149562
144.354680	3306.928394	6.318195	-0.029223	3.153186
144.619707	3314.971961	6.323200	-0.029278	3.156798
144.780758	3322.965137	6.328205	-0.029313	3.160379
145.164804	3330.975196	6.333210	-0.029390	3.163974
145.091110	3339.030502	6.338214	-0.029382	3.167564
145.303676	3347.081265	6.343219	-0.029427	3.171161
145.688252	3355.115564	6.348224	-0.029504	3.174754
145.769507	3363.141296	6.353229	-0.029525	3.178326
145.826981	3371.198788	6.358234	-0.029541	3.181907
146.028603	3379.183969	6.363238	-0.029584	3.185458
146.518783	3387.211180	6.368243	-0.029681	3.189035
146.865094	3395.268455	6.373248	-0.029751	3.192616
146.899140	3403.316673	6.378253	-0.029763	3.196176
147.190266	3411.321142	6.383258	-0.029822	3.199723
147.244105	3419.324595	6.388262	-0.029838	3.203256
147.459497	3427.376200	6.393267	-0.029883	3.206813
147.716198	3435.403147	6.398272	-0.029937	3.210357
147.907367	3443.463042	6.403277	-0.029978	3.213908
148.048403	3451.501111	6.408282	-0.030009	3.217444
148.316668	3459.514073	6.413286	-0.030065	3.220971
148.537940	3467.491175	6.418291	-0.030111	3.224476
148.772700	3475.559304	6.423296	-0.030161	3.228017
148.898092	3483.620909	6.428301	-0.030190	3.231547
149.171706	3491.714779	6.433306	-0.030246	3.235093
149.368647	3499.678742	6.438310	-0.030288	3.238576
149.676473	3507.691265	6.443315	-0.030351	3.242080
150.083654	3515.704136	6.448320	-0.030432	3.245585
150.308224	3523.704674	6.453325	-0.030479	3.249073
150.410213	3531.798577	6.458330	-0.030504	3.252593
150.545899	3539.842055	6.463334	-0.030535	3.256089
150.777962	3547.812618	6.468339	-0.030583	3.259553
151.229379	3555.851764	6.473344	-0.030673	3.263052
151.254115	3563.880272	6.478349	-0.030683	3.266525
151.516020	3571.913786	6.483354	-0.030737	3.270007
151.953145	3579.949456	6.488358	-0.030824	3.273492
152.006036	3587.980267	6.493363	-0.030839	3.276957
152.131139	3596.023220	6.498368	-0.030868	3.280426
152.488909	3603.976750	6.503373	-0.030940	3.283861
152.744942	3612.056267	6.508378	-0.030993	3.287344
152.656859	3620.098346	6.513382	-0.030982	3.290793
152.804583	3628.153132	6.518387	-0.031015	3.294253
153.126403	3636.190648	6.523392	-0.031081	3.297709
153.099978	3644.202954	6.528397	-0.031081	3.301137
153.584691	3652.190375	6.533402	-0.031177	3.304570
153.884588	3660.229869	6.538406	-0.031238	3.308015
154.018377	3668.306571	6.543411	-0.031269	3.311465
154.238720	3676.369435	6.548416	-0.031315	3.314910
154.387686	3684.327518	6.553421	-0.031349	3.318304
154.959274	3692.348322	6.558426	-0.031460	3.321736
155.234921	3700.351575	6.563430	-0.031517	3.325147
155.425657	3708.389049	6.568435	-0.031558	3.328565
155.891346	3716.429924	6.573440	-0.031650	3.331991
155.921148	3724.482052	6.578445	-0.031661	3.335403
155.962534	3732.525192	6.583450	-0.031675	3.338807
156.157155	3740.530701	6.588454	-0.031716	3.342198
156.443505	3748.522411	6.593459	-0.031775	3.345583
156.495251	3756.592323	6.598464	-0.031790	3.348989
156.688538	3764.630805	6.603469	-0.031832	3.352383
157.061582	3772.685017	6.608474	-0.031907	3.355787
157.098576	3780.665864	6.613478	-0.031919	3.359144
157.262168	3788.696631	6.618483	-0.031955	3.362524
157.621272	3796.721773	6.623488	-0.032027	3.365905
157.622026	3804.726965	6.628493	-0.032033	3.369261
158.046908	3812.794927	6.633498	-0.032118	3.372655
158.191720	3820.851035	6.638502	-0.032150	3.376031
158.607038	3828.836994	6.643507	-0.032233	3.379384
158.671211	3836.885546	6.648512	-0.032250	3.382747
158.797079	3844.904728	6.653517	-0.032279	3.386096
159.206220	3852.911758	6.658522	-0.032361	3.389447
159.145750	3861.017475	6.663526	-0.032355	3.392820
159.330057	3869.084388	6.668531	-0.032395	3.396181
159.687344	3877.033625	6.673536	-0.032467	3.399497
159.838912	3885.004236	6.678541	-0.032500	3.402810
160.010016	3893.051872	6.683546	-0.032538	3.406153
160.160444	3901.045133	6.688550	-0.032571	3.409470
160.523879	3909.086684	6.693555	-0.032644	3.412810
160.417942	3917.181218	6.698560	-0.032630	3.416153
160.597784	3925.142807	6.703565	-0.032669	3.419448
160.887700	3933.167431	6.708570	-0.032729	3.422769
161.024493	3941.220166	6.713574	-0.032760	3.426094
161.293965	3949.217573	6.718579	-0.032815	3.429396
161.886706	3957.287462	6.723584	-0.032931	3.432737
161.991214	3965.312660	6.728589	-0.032956	3.436039
162.236249	3973.319733	6.733594	-0.033007	3.439335
162.447340	3981.338891	6.738598	-0.033052	3.442632
162.762476	3989.339877	6.743603	-0.033116	3.445921
163.086840	3997.391400	6.748608	-0.033182	3.449229
163.175873	4005.425512	6.753613	-0.033204	3.452518
163.412796	4013.511990	6.758618	-0.033254	3.455831
163.495310	4021.496335	6.763622	-0.033274	3.459093
163.685730	4029.515611	6.768627	-0.033315	3.462370
163.893239	4037.532783	6.773632	-0.033359	3.465644
164.016212	4045.574354	6.778637	-0.033388	3.468922
164.218046	4053.641131	6.783642	-0.033431	3.472209
164.422488	4061.666251	6.788646	-0.033474	3.475477
164.666927	4069.648926	6.793651	-0.033525	3.478725
165.005786	4077.660995	6.798656	-0.033594	3.481986
165.084794	4085.658801	6.803661	-0.033614	3.485229
165.452768	4093.698502	6.808666	-0.033688	3.488495
165.592518	4101.748351	6.813670	-0.033720	3.491755
165.678276	4109.771363	6.818675	-0.033741	3.494999
166.025675	4117.802370	6.823680	-0.033811	3.498252
166.102692	4125.803960	6.828685	-0.033831	3.501481
166.358646	4133.820030	6.833690	-0.033884	3.504719
166.640939	4141.859447	6.838694	-0.033942	3.507964
166.793808	4149.896243	6.843699	-0.033976	3.511201
167.002475	4157.945566	6.848704	-0.034020	3.514442
167.073046	4165.962451	6.853709	-0.034039	3.517662
167.313890	4173.995485	6.858714	-0.034089	3.520891
167.526442	4181.941513	6.863718	-0.034134	3.524082
167.467241	4190.021669	6.868723	-0.034129	3.527314
167.848154	4198.069515	6.873728	-0.034205	3.530545
168.137408	4206.051351	6.878733	-0.034265	3.533743
168.365788	4214.123401	6.883738	-0.034313	3.536972
168.621544	4222.158589	6.888742	-0.034366	3.540185
168.901370	4230.128060	6.893747	-0.034423	3.543369
169.134976	4238.189111	6.898752	-0.034472	3.546585
169.389872	4246.185327	6.903757	-0.034525	3.549774
169.656022	4254.316130	6.908762	-0.034580	3.553013
169.679532	4262.361625	6.913766	-0.034590	3.556208
169.921785	4270.313878	6.918771	-0.034641	3.559369
170.071740	4278.333747	6.923776	-0.034674	3.562552
170.156936	4286.330151	6.928781	-0.034695	3.565721
170.256347	4294.363458	6.933786	-0.034719	3.568902
170.317884	4302.390173	6.938790	-0.034736	3.572077
170.766797	4310.407538	6.943795	-0.034825	3.575256
170.991031	4318.421758	6.948800	-0.034873	3.578424
170.907490	4326.468796	6.953805	-0.034862	3.581594
171.150676	4334.450010	6.958810	-0.034913	3.584744
171.212054	4342.499964	6.963814	-0.034930	3.587914
171.385900	4350.531460	6.968819	-0.034968	3.591076
171.784598	4358.557881	6.973824	-0.035048	3.594241
171.955660	4366.546657	6.978829	-0.035085	3.597381
172.156708	4374.572208	6.983834	-0.035128	3.600533
172.410040	4382.570059	6.988838	-0.035180	3.603674
172.758012	4390.605760	6.993843	-0.035251	3.606829
172.753037	4398.649814	6.998848	-0.035255	3.609975
173.027118	4406.673896	7.003853	-0.035312	3.613117
173.283253	4414.727968	7.008858	-0.035365	3.616269
173.340688	4422.714325	7.013862	-0.035381	3.619385
173.365386	4430.745968	7.018867	-0.035391	3.622516
173.666574	4438.776405	7.023872	-0.035453	3.625651
173.714065	4446.800379	7.028877	-0.035467	3.628774
173.878261	4454.883416	7.033882	-0.035503	3.631921
174.070790	4462.906428	7.038886	-0.035544	3.635042
174.291393	4470.895041	7.043891	-0.035591	3.638147
174.543347	4478.942393	7.048896	-0.035643	3.641274
174.753313	4486.860187	7.053901	-0.035688	3.644347
175.017346	4494.948094	7.058906	-0.035743	3.647484
175.140828	4502.967926	7.063910	-0.035771	3.650589
175.212516	4511.024868	7.068915	-0.035790	3.653703
175.423642	4519.067885	7.073920	-0.035835	3.656814
175.674169	4527.032574	7.078925	-0.035887	3.659893
175.949800	4535.059119	7.083930	-0.035944	3.662993
176.134372	4543.117411	7.088934	-0.035983	3.666101
176.118705	4551.110080	7.093939	-0.035986	3.669175
176.611716	4559.162997	7.098944	-0.036083	3.672283
176.782337	4567.191724	7.103949	-0.036120	3.675371
176.960506	4575.189343	7.108954	-0.036159	3.678445
177.203283	4583.216311	7.113958	-0.036210	3.681529
177.350412	4591.197784	7.118963	-0.036243	3.684590
177.495911	4599.278280	7.123968	-0.036275	3.687687
177.594356	4607.299334	7.128973	-0.036299	3.690757
177.831696	4615.311428	7.133978	-0.036349	3.693825
178.107478	4623.347403	7.138982	-0.036406	3.696900
178.214498	4631.313651	7.143987	-0.036431	3.699942
178.674912	4639.334718	7.148992	-0.036522	3.703011
178.903065	4647.389254	7.153997	-0.036570	3.706084
178.947003	4655.410836	7.159002	-0.036584	3.709138
178.918006	4663.495526	7.164006	-0.036584	3.712211
179.369518	4671.541109	7.169011	-0.036673	3.715279
179.649858	4679.517343	7.174016	-0.036731	3.718313
179.689422	4687.527195	7.179021	-0.036744	3.721352
179.721264	4695.520213	7.184026	-0.036755	3.724382
179.927277	4703.519381	7.189030	-0.036799	3.727416
180.094730	4711.554857	7.194035	-0.036836	3.730460
180.426026	4719.583293	7.199040	-0.036903	3.733503
180.655445	4727.586832	7.204045	-0.036951	3.736532
180.986129	4735.595563	7.209050	-0.037018	3.739563
181.055972	4743.644709	7.214054	-0.037037	3.742600
181.162886	4751.652524	7.219059	-0.037062	3.745620
181.378303	4759.685803	7.224064	-0.037108	3.748649
181.548653	4767.739280	7.229069	-0.037145	3.751683
181.878525	4775.785314	7.234074	-0.037212	3.754715
181.840441	4783.794217	7.239078	-0.037210	3.757722
182.123624	4791.811373	7.244083	-0.037268	3.760737
182.272266	4799.805876	7.249088	-0.037301	3.763738
182.281445	4807.862884	7.254093	-0.037309	3.766757
182.255114	4815.889325	7.259098	-0.037309	3.769762
182.700106	4823.911864	7.264102	-0.037397	3.772773
182.997770	4831.923209	7.269107	-0.037458	3.775774
182.908098	4839.977856	7.274112	-0.037447	3.778780
182.937798	4847.999053	7.279117	-0.037458	3.781774
183.263423	4855.971165	7.284122	-0.037524	3.784754
183.518306	4863.989990	7.289126	-0.037577	3.787748
183.739185	4872.023178	7.294131	-0.037624	3.790743
184.058369	4880.098961	7.299136	-0.037689	3.793754
184.049066	4888.118427	7.304141	-0.037692	3.796735
184.299366	4896.050657	7.309146	-0.037744	3.799686
184.814072	4904.106575	7.314150	-0.037846	3.802687
184.861393	4912.097128	7.319155	-0.037860	3.805651
185.002500	4920.163475	7.324160	-0.037892	3.808643
184.943688	4928.199802	7.329165	-0.037886	3.811617
185.295426	4936.199962	7.334170	-0.037957	3.814584
185.721504	4944.210656	7.339174	-0.038042	3.817555
185.613183	4952.215497	7.344179	-0.038027	3.820509
185.897264	4960.234390	7.349184	-0.038086	3.823475
185.991339	4968.268837	7.354189	-0.038109	3.826440
186.104257	4976.256787	7.359194	-0.038135	3.829385
186.379331	4984.337561	7.364198	-0.038192	3.832367
186.593162	4992.337400	7.369203	-0.038237	3.835314
186.697862	5000.382795	7.374208	-0.038262	3.838274
186.987901	5008.342392	7.379213	-0.038322	3.841204
187.230318	5016.344906	7.384218	-0.038372	3.844147
187.346081	5024.406734	7.389222	-0.038399	3.847106
187.666101	5032.415716	7.394227	-0.038464	3.850048
187.925948	5040.487189	7.399232	-0.038518	3.853009
187.809524	5048.527789	7.404237	-0.038502	3.855949
188.109917	5056.534401	7.409242	-0.038563	3.858883
188.445946	5064.531608	7.414246	-0.038631	3.861812
188.309566	5072.559210	7.419251	-0.038611	3.864740
188.470470	5080.616855	7.424256	-0.038647	3.867683
188.609934	5088.598776	7.429261	-0.038678	3.870595
188.926703	5096.848108	7.434266	-0.038743	3.873606
189.200011	5104.849787	7.439270	-0.038799	3.876524
188.851529	5112.753684	7.444275	-0.038740	3.879392
189.104418	5120.735883	7.449280	-0.038792	3.882298
189.353625	5128.707176	7.454285	-0.038844	3.885198
189.480268	5136.733235	7.459290	-0.038873	3.888113
189.701112	5144.776748	7.464294	-0.038920	3.891034
189.929593	5152.786354	7.469299	-0.038968	3.893940
190.162911	5160.817322	7.474304	-0.039017	3.896853
190.139945	5168.791883	7.479309	-0.039018	3.899737
190.549125	5176.832697	7.484314	-0.039100	3.902652
190.764525	5184.848295	7.489318	-0.039145	3.905552
190.708144	5192.845115	7.494323	-0.039140	3.908437
191.053232	5200.885092	7.499328	-0.039210	3.911344
191.346053	5208.918300	7.504333	-0.039270	3.914245
191.324673	5216.959840	7.509338	-0.039271	3.917141
191.614245	5224.925493	7.514342	-0.039331	3.920013
191.890977	5232.910798	7.519347	-0.039388	3.922890
191.973419	5240.997979	7.524352	-0.039409	3.925798
191.854133	5248.991804	7.529357	-0.039392	3.928666
192.177951	5257.016133	7.534362	-0.039458	3.931552
192.303768	5265.057298	7.539366	-0.039486	3.934437
192.312252	5273.051014	7.544371	-0.039494	3.937302
192.881272	5281.079386	7.549376	-0.039605	3.940187
193.145699	5289.069622	7.554381	-0.039660	3.943050
193.141645	5297.134939	7.559386	-0.039664	3.945934
193.428163	5305.149921	7.564390	-0.039723	3.948802
193.618811	5313.167680	7.569395	-0.039764	3.951668
193.832412	5321.229625	7.574400	-0.039809	3.954547
193.688417	5329.213280	7.579405	-0.039788	3.957391
193.888971	5337.207879	7.584410	-0.039831	3.960242
194.089977	5345.211820	7.589414	-0.039874	3.963095
194.198945	5353.231304	7.594419	-0.039900	3.965949
194.668332	5361.222704	7.599424	-0.039992	3.968798
194.741437	5369.271443	7.604429	-0.040011	3.971658
195.042149	5377.329315	7.609434	-0.040073	3.974523
194.961241	5385.357433	7.614438	-0.040063	3.977369
195.155650	5393.311364	7.619443	-0.040105	3.980191
195.507033	5401.364211	7.624448	-0.040176	3.983049
195.580247	5409.385663	7.629453	-0.040195	3.985889
195.896677	5417.387457	7.634458	-0.040259	3.988724
196.206742	5425.456357	7.639462	-0.040323	3.991581
196.314309	5433.494509	7.644467	-0.040348	3.994421
196.535102	5441.522627	7.649472	-0.040395	3.997258
196.726286	5449.499448	7.654477	-0.040436	4.000074
196.717660	5457.542461	7.659482	-0.040440	4.002908
196.844964	5465.555760	7.664486	-0.040469	4.005732
197.036635	5473.547025	7.669491	-0.040510	4.008547
197.307766	5481.635464	7.674496	-0.040566	4.011396
197.457176	5489.631223	7.679501	-0.040599	4.014208
197.557006	5497.675776	7.684506	-0.040623	4.017034
197.975704	5505.665646	7.689510	-0.040707	4.019844
198.101244	5513.647492	7.694515	-0.040736	4.022645
198.440056	5521.687992	7.699520	-0.040804	4.025468
198.531568	5529.717441	7.704525	-0.040827	4.028280
198.838877	5537.772618	7.709530	-0.040889	4.031104
198.801400	5545.885128	7.714534	-0.040888	4.033940
198.984874	5553.841866	7.719539	-0.040927	4.036723
199.485612	5561.797722	7.724544	-0.041026	4.039508
199.308465	5569.822253	7.729549	-0.040999	4.042305
199.460271	5577.799775	7.734554	-0.041032	4.045089
199.659276	5585.877668	7.739558	-0.041075	4.047907
199.682450	5593.861953	7.744563	-0.041085	4.050687
200.089194	5601.913742	7.749568	-0.041166	4.053495
200.279765	5609.923731	7.754573	-0.041207	4.056283
200.749231	5617.877398	7.759578	-0.041300	4.059053
200.784301	5625.973389	7.764582	-0.041312	4.061865
200.943259	5633.928606	7.769587	-0.041347	4.064628
201.287879	5641.982579	7.774592	-0.041416	4.067425
201.335549	5649.966929	7.779597	-0.041431	4.070193
201.507978	5658.032850	7.784602	-0.041468	4.072988
201.725282	5666.084531	7.789606	-0.041514	4.075777
201.845460	5674.019286	7.794611	-0.041542	4.078523
202.104504	5682.076806	7.799616	-0.041596	4.081311
202.344858	5690.047541	7.804621	-0.041646	4.084067
202.376485	5698.124344	7.809626	-0.041657	4.086854
202.701500	5706.090976	7.814630	-0.041723	4.089606
202.737056	5714.130651	7.819635	-0.041735	4.092377
203.031080	5722.186573	7.824640	-0.041796	4.095155
203.014590	5730.171217	7.829645	-0.041798	4.097903
203.101917	5738.179913	7.834650	-0.041820	4.100658
203.415684	5746.238951	7.839654	-0.041884	4.103432
203.631733	5754.222750	7.844659	-0.041929	4.106177
203.637704	5762.301875	7.849664	-0.041936	4.108950
203.709041	5770.298401	7.854669	-0.041955	4.111694
204.080386	5778.329102	7.859674	-0.042029	4.114451
204.052057	5786.357528	7.864678	-0.042030	4.117201
204.080015	5794.285206	7.869683	-0.042040	4.119915
204.739102	5802.351773	7.874688	-0.042168	4.122682
204.934470	5810.315973	7.879693	-0.042210	4.125407
204.667592	5818.378363	7.884698	-0.042166	4.128158
204.747022	5826.427904	7.889702	-0.042186	4.130907
205.074258	5834.440900	7.894707	-0.042253	4.133645
205.244765	5842.517224	7.899712	-0.042290	4.136400
205.320228	5850.464921	7.904717	-0.042309	4.139109
205.379576	5858.503746	7.909722	-0.042326	4.141846
205.701840	5866.485348	7.914726	-0.042391	4.144566
205.754995	5874.534192	7.919731	-0.042407	4.147303
205.754268	5882.581085	7.924736	-0.042412	4.150038
206.210330	5890.584228	7.929741	-0.042502	4.152761
206.288357	5898.660250	7.934746	-0.042523	4.155502
206.380813	5906.626029	7.939750	-0.042545	4.158204
206.636454	5914.615392	7.944755	-0.042598	4.160915
206.652333	5922.625641	7.949760	-0.042607	4.163628
206.783586	5930.651976	7.954765	-0.042637	4.166346
207.262238	5938.660807	7.959770	-0.042731	4.169060
207.213192	5946.732504	7.964774	-0.042727	4.171788
207.330468	5954.732729	7.969779	-0.042755	4.174492
207.637402	5962.782790	7.974784	-0.042817	4.177212
207.933532	5970.746012	7.979789	-0.042878	4.179902
207.945400	5978.764572	7.984794	-0.042886	4.182605
208.297398	5986.754073	7.989798	-0.042957	4.185301
208.358725	5994.796325	7.994803	-0.042974	4.188009
208.812685	6002.838599	7.999808	-0.043064	4.190720
208.679493	6010.932001	8.004813	-0.043044	4.193440
208.981265	6018.952646	8.009818	-0.043106	4.196138
209.241890	6026.902696	8.014822	-0.043160	4.198811
209.240223	6034.888500	8.019827	-0.043165	4.201491
209.496372	6042.875085	8.024832	-0.043218	4.204172
209.438068	6050.904592	8.029837	-0.043213	4.206862
209.582711	6058.915250	8.034842	-0.043245	4.209547
209.914743	6066.980394	8.039846	-0.043313	4.212250
209.937569	6074.966916	8.044851	-0.043322	4.214922
210.078929	6083.025003	8.049856	-0.043354	4.217617
210.318274	6090.954492	8.054861	-0.043404	4.220269
210.391143	6099.007227	8.059866	-0.043423	4.222958
210.631360	6107.017113	8.064870	-0.043473	4.225633
210.843157	6115.018032	8.069875	-0.043518	4.228303
211.047920	6123.082414	8.074880	-0.043562	4.230992
211.177567	6131.111065	8.079885	-0.043591	4.233667
211.345026	6139.152208	8.084890	-0.043628	4.236345
211.320461	6147.145808	8.089894	-0.043629	4.239003
211.470383	6155.160121	8.094899	-0.043662	4.241668
211.778490	6163.114896	8.099904	-0.043725	4.244314
211.911541	6171.166237	8.104909	-0.043755	4.246988
211.976326	6179.193556	8.109914	-0.043773	4.249651
212.117031	6187.251158	8.114918	-0.043805	4.252324
212.009458	6195.240612	8.119923	-0.043790	4.254970
212.543206	6203.316505	8.124928	-0.043895	4.257649
212.630055	6211.274883	8.129933	-0.043917	4.260284
212.718292	6219.315627	8.134938	-0.043938	4.262944
212.798272	6227.327641	8.139942	-0.043959	4.265592
213.130126	6235.331368	8.144947	-0.044026	4.268239
213.295826	6243.381484	8.149952	-0.044062	4.270898
213.509229	6251.484671	8.154957	-0.044108	4.273572
213.539402	6259.483166	8.159962	-0.044119	4.276210
213.726734	6267.422851	8.164966	-0.044159	4.278827
213.811709	6275.452617	8.169971	-0.044180	4.281472
214.116191	6283.424873	8.174976	-0.044242	4.284098
214.187519	6291.476400	8.179981	-0.044261	4.286746
214.167227	6299.439260	8.184986	-0.044263	4.289363
214.382967	6307.556111	8.189990	-0.044309	4.292031
214.477544	6315.506981	8.194995	-0.044332	4.294641
214.742810	6323.583279	8.200000	-0.044387	4.297293
214.823093	6331.546277	8.205005	-0.044407	4.299904
214.978032	6339.594335	8.210010	-0.044441	4.302542
215.226383	6347.607981	8.215014	-0.044493	4.305168
215.042473	6355.603441	8.220019	-0.044464	4.307783
215.413079	6363.643217	8.225024	-0.044539	4.310415
215.476599	6371.642650	8.230029	-0.044556	4.313030
215.526136	6379.654942	8.235034	-0.044571	4.315648
215.984030	6387.688624	8.240038	-0.044661	4.318274
216.055255	6395.679671	8.245043	-0.044680	4.320881
216.124802	6403.723513	8.250048	-0.044698	4.323504
216.350257	6411.721840	8.255053	-0.044746	4.326112
216.659641	6419.723240	8.260058	-0.044809	4.328720
216.957598	6427.800858	8.265062	-0.044870	4.331351
216.791651	6435.776432	8.270067	-0.044845	4.333944
216.800966	6443.843270	8.275072	-0.044852	4.336566
217.060395	6451.805849	8.280077	-0.044905	4.339154
217.148268	6459.830782	8.285082	-0.044927	4.341760
217.305519	6467.794642	8.290086	-0.044962	4.344345
217.491675	6475.853248	8.295091	-0.045002	4.346960
217.782678	6483.881872	8.300096	-0.045062	4.349563
218.067279	6491.957989	8.305101	-0.045120	4.352181
218.097523	6499.988250	8.310106	-0.045131	4.354780
218.352977	6508.015944	8.315110	-0.045185	4.357379
218.700266	6515.928875	8.320115	-0.045255	4.359939
218.832694	6523.956160	8.325120	-0.045285	4.362533
218.823646	6531.947500	8.330125	-0.045288	4.365114
218.815750	6539.984196	8.335130	-0.045292	4.367707
219.048196	6547.991099	8.340134	-0.045341	4.370291
219.440099	6555.971750	8.345139	-0.045420	4.372866
219.752710	6564.069263	8.350144	-0.045483	4.375476
219.762388	6572.069636	8.355149	-0.045491	4.378052
219.782637	6580.059009	8.360154	-0.045500	4.380622
220.141509	6588.090705	8.365158	-0.045572	4.383207
220.254350	6596.092799	8.370163	-0.045599	4.385779
220.516776	6604.104791	8.375168	-0.045653	4.388354
220.625546	6612.117464	8.380173	-0.045679	4.390926
220.724821	6620.140893	8.385178	-0.045703	4.393501
220.941291	6628.236241	8.390182	-0.045748	4.396097
220.951599	6636.161575	8.395187	-0.045756	4.398637
221.318512	6644.216253	8.400192	-0.045830	4.401218
221.571031	6652.169380	8.405197	-0.045882	4.403765
221.554329	6660.251683	8.410202	-0.045884	4.406350
221.826067	6668.275490	8.415206	-0.045940	4.408916
222.123036	6676.290982	8.420211	-0.046001	4.411478
222.182872	6684.324752	8.425216	-0.046018	4.414044
222.278515	6692.352887	8.430221	-0.046041	4.416606
222.371873	6700.292738	8.435226	-0.046064	4.419138
222.690831	6708.380761	8.440230	-0.046129	4.421718
222.648737	6716.352540	8.445235	-0.046126	4.424257
222.984065	6724.411638	8.450240	-0.046194	4.426824
223.099065	6732.411021	8.455245	-0.046221	4.429370
223.219077	6740.482753	8.460250	-0.046249	4.431937
223.344963	6748.522779	8.465254	-0.046278	4.434493
223.463964	6756.501720	8.470259	-0.046306	4.437027
223.627087	6764.494513	8.475264	-0.046341	4.439565
223.994283	6772.498055	8.480269	-0.046415	4.442106
224.239897	6780.447870	8.485274	-0.046466	4.444628
224.358203	6788.580381	8.490278	-0.046494	4.447205
224.314885	6796.512676	8.495283	-0.046491	4.449717
224.466453	6804.610747	8.500288	-0.046525	4.452281
224.616189	6812.588200	8.505293	-0.046558	4.454805
224.886991	6820.654689	8.510298	-0.046614	4.457356
224.960352	6828.634419	8.515302	-0.046633	4.459878
224.824315	6836.649883	8.520307	-0.046614	4.462409
225.033010	6844.616325	8.525312	-0.046658	4.464924
225.151574	6852.667595	8.530317	-0.046685	4.467464
225.318068	6860.647671	8.535322	-0.046722	4.469980
225.473022	6868.736520	8.540326	-0.046756	4.472529
225.526051	6876.724064	8.545331	-0.046772	4.475045
225.865153	6884.737855	8.550336	-0.046840	4.477568
225.964909	6892.721113	8.555341	-0.046864	4.480079
226.087784	6900.783164	8.560346	-0.046893	4.482614
226.276767	6908.722925	8.565351	-0.046933	4.485109
226.649895	6916.790661	8.570355	-0.047008	4.487644
226.539001	6924.793226	8.575360	-0.046993	4.490155
226.787057	6932.846569	8.580365	-0.047045	4.492681
226.781253	6940.839198	8.585370	-0.047049	4.495187
227.044772	6948.875674	8.590375	-0.047104	4.497705
227.026981	6956.827549	8.595379	-0.047106	4.500195
227.303653	6964.900977	8.600384	-0.047163	4.502722
227.566988	6972.870340	8.605389	-0.047217	4.505215
227.717659	6980.895131	8.610394	-0.047251	4.507724
228.146053	6988.929168	8.615399	-0.047336	4.510235
228.074445	6997.009893	8.620403	-0.047328	4.512758
228.252415	7005.057132	8.625408	-0.047367	4.515270
228.336596	7013.036555	8.630413	-0.047388	4.517759
228.464558	7020.947959	8.635418	-0.047417	4.520225
228.589347	7029.002095	8.640423	-0.047446	4.522735
228.370709	7037.002015	8.645427	-0.047411	4.525225
228.757256	7045.023168	8.650432	-0.047488	4.527722
228.936333	7053.016160	8.655437	-0.047527	4.530208
229.037970	7061.038236	8.660442	-0.047551	4.532702
229.186601	7069.099663	8.665447	-0.047584	4.535207
229.285278	7077.084454	8.670451	-0.047608	4.537686
229.527132	7085.097970	8.675456	-0.047659	4.540174
229.477240	7093.104562	8.680461	-0.047655	4.542657
229.656839	7101.098138	8.685466	-0.047694	4.545135
229.912750	7109.145138	8.690471	-0.047747	4.547629
229.868669	7117.145762	8.695475	-0.047744	4.550106
230.012388	7125.240625	8.700480	-0.047776	4.552611
230.159191	7133.270333	8.705485	-0.047809	4.555095
230.335411	7141.233643	8.710490	-0.047847	4.557557
230.707989	7149.248995	8.715495	-0.047922	4.560034
230.601501	7157.257707	8.720499	-0.047908	4.562507
230.745648	7165.267713	8.725504	-0.047940	4.564980
230.852913	7173.313649	8.730509	-0.047966	4.567462
230.984656	7181.274784	8.735514	-0.047996	4.569916
231.171181	7189.340410	8.740519	-0.048036	4.572402
230.984656	7197.334628	8.745523	-0.048007	4.574863
231.196995	7205.397842	8.750528	-0.048052	4.577345
231.420407	7213.343673	8.755533	-0.048099	4.579790
231.401071	7221.377766	8.760538	-0.048101	4.582260
231.641948	7229.408453	8.765543	-0.048151	4.584728
232.014312	7237.440227	8.770547	-0.048226	4.587195
231.902412	7245.468302	8.775552	-0.048210	4.589659
232.111373	7253.523482	8.780557	-0.048255	4.592130
232.287516	7261.508797	8.785562	-0.048293	4.594579
232.569167	7269.581857	8.790567	-0.048351	4.597053
232.600784	7277.466997	8.795571	-0.048362	4.599468
232.762879	7285.588748	8.800576	-0.048398	4.601955
232.932662	7293.497557	8.805581	-0.048435	4.604375
232.976512	7301.540375	8.810586	-0.048449	4.606834
233.080921	7309.586467	8.815591	-0.048473	4.609293
233.133564	7317.609317	8.820595	-0.048489	4.611744
233.408822	7325.652812	8.825600	-0.048546	4.614200
233.627288	7333.672047	8.830605	-0.048592	4.616647
233.702649	7341.634148	8.835610	-0.048611	4.619075
233.738497	7349.687536	8.840615	-0.048623	4.621530
233.928364	7357.614134	8.845619	-0.048664	4.623945
233.916077	7365.685279	8.850624	-0.048667	4.626402
234.064440	7373.703432	8.855629	-0.048700	4.628843
234.309473	7381.744486	8.860634	-0.048751	4.631288
234.363242	7389.805019	8.865639	-0.048767	4.633739
234.398736	7397.787597	8.870643	-0.048779	4.636164
234.765387	7405.729752	8.875648	-0.048853	4.638576
234.771525	7413.776272	8.880653	-0.048859	4.641018
234.805967	7421.767402	8.885658	-0.048871	4.643443
235.209507	7429.843969	8.890663	-0.048952	4.645891
235.308254	7437.786071	8.895667	-0.048976	4.648298
235.440294	7445.834500	8.900672	-0.049006	4.650736
235.409939	7453.880529	8.905677	-0.049006	4.653171
235.639914	7461.897553	8.910682	-0.049054	4.655597
235.573069	7469.919902	8.915687	-0.049047	4.658023
235.607556	7477.868263	8.920691	-0.049059	4.660425
235.855278	7485.926998	8.925696	-0.049110	4.662860
235.973231	7493.935748	8.930701	-0.049138	4.665278
236.162507	7501.949006	8.935706	-0.049178	4.667696
236.524685	7509.964155	8.940711	-0.049251	4.670113
236.539513	7518.057629	8.945715	-0.049260	4.672553
236.728030	7526.123015	8.950720	-0.049300	4.674982
236.941480	7534.025849	8.955725	-0.049345	4.677362
236.941457	7541.976304	8.960730	-0.049351	4.679755
237.132373	7550.059543	8.965735	-0.049392	4.682186
237.173646	7557.977981	8.970739	-0.049405	4.684567
237.209450	7566.073972	8.975744	-0.049417	4.687000
237.413737	7574.109698	8.980749	-0.049461	4.689414
237.475281	7582.112365	8.985754	-0.049478	4.691816
237.797296	7590.105208	8.990759	-0.049543	4.694214
237.785346	7598.132365	8.995763	-0.049546	4.696621
237.807275	7606.098239	9.000768	-0.049556	4.699009
237.906264	7614.151059	9.005773	-0.049580	4.701421
238.179141	7622.111271	9.010778	-0.049636	4.703804
238.346242	7630.194851	9.015783	-0.049673	4.706223
238.245597	7638.203398	9.020787	-0.049659	4.708619
238.664049	7646.233574	9.025792	-0.049743	4.711019
238.783433	7654.275056	9.030797	-0.049770	4.713421
238.682421	7662.261404	9.035802	-0.049757	4.715807
238.859141	7670.254069	9.040807	-0.049795	4.718193
239.012255	7678.269494	9.045811	-0.049829	4.720584
239.147078	7686.256430	9.050816	-0.049860	4.722965
239.351537	7694.287887	9.055821	-0.049903	4.725358
239.439609	7702.323496	9.060826	-0.049925	4.727752
239.670513	7710.359299	9.065831	-0.049974	4.730144
239.295549	7718.389338	9.070835	-0.049909	4.732535
239.752977	7726.443937	9.075840	-0.050000	4.734930
239.896325	7734.457690	9.080845	-0.050032	4.737312
239.881393	7742.416149	9.085850	-0.050035	4.739677
240.341102	7750.447583	9.090855	-0.050126	4.742061
240.346399	7758.390137	9.095859	-0.050132	4.744418
240.283382	7766.479066	9.100864	-0.050126	4.746818
240.495289	7774.463427	9.105869	-0.050171	4.749186
240.739945	7782.484882	9.110874	-0.050222	4.751562
240.843457	7790.562632	9.115879	-0.050247	4.753955
240.898217	7798.557465	9.120883	-0.050263	4.756322
241.163298	7806.521819	9.125888	-0.050317	4.758678
241.217787	7814.556365	9.130893	-0.050333	4.761055
241.226376	7822.516245	9.135898	-0.050340	4.763408
241.438007	7830.587164	9.140903	-0.050385	4.765792
241.527577	7838.561319	9.145907	-0.050407	4.768147
241.773110	7846.586906	9.150912	-0.050458	4.770516
241.894470	7854.655215	9.155917	-0.050486	4.772896
242.175702	7862.668265	9.160922	-0.050544	4.775258
242.293965	7870.640878	9.165927	-0.050572	4.777608
242.286039	7878.641222	9.170931	-0.050576	4.779965
242.503351	7886.713259	9.175936	-0.050622	4.782341
242.472218	7894.659732	9.180941	-0.050621	4.784680
242.334836	7902.692468	9.185946	-0.050601	4.787044
242.710353	7910.721509	9.190951	-0.050676	4.789403
242.880811	7918.751723	9.195955	-0.050714	4.791762
243.095213	7926.749399	9.200960	-0.050759	4.794111
242.943907	7934.815903	9.205965	-0.050736	4.796480
243.154429	7942.747019	9.210970	-0.050781	4.798806
243.572112	7950.839577	9.215975	-0.050864	4.801178
243.446499	7958.773539	9.220979	-0.050846	4.803504
243.639979	7966.850531	9.225984	-0.050888	4.805870
243.801506	7974.805269	9.230989	-0.050923	4.808199
244.009822	7982.812680	9.235994	-0.050968	4.810542
244.110265	7990.315394	9.240999	-0.050991	4.812737
243.862324	7994.823318	9.246003	-0.050948	4.814057

244.260139	7997.170019	9.251008	-0.051024	4.814741
244.170002	7998.605769	9.256013	-0.051009	4.815161
244.427781	7999.053129	9.261018	-0.051057	4.815291
244.562701	7999.811392	9.266023	-0.051083	4.815512
244.485446	7999.759964	9.271027	-0.051069	4.815497
244.667300	7999.803528	9.276032	-0.051103	4.815509
244.816494	7999.807049	9.281037	-0.051131	4.815509
244.668608	7999.777963	9.286042	-0.051104	4.815502
244.533424	7999.765102	9.291047	-0.051079	4.815498
244.677865	7999.809125	9.296051	-0.051106	4.815511
244.796936	7999.811087	9.301056	-0.051128	4.815511
244.823469	7999.777368	9.306061	-0.051134	4.815501
244.788566	7999.706340	9.311066	-0.051127	4.815480
245.080096	7999.784798	9.316071	-0.051182	4.815502
244.895527	7999.749774	9.321075	-0.051148	4.815492
244.936146	7999.740846	9.326080	-0.051155	4.815489
244.943061	7999.787967	9.331085	-0.051157	4.815503
244.964407	7999.761639	9.336090	-0.051161	4.815495
245.062727	7999.779282	9.341095	-0.051180	4.815500
245.074683	7999.763479	9.346099	-0.051182	4.815495
245.326808	7999.872266	9.351104	-0.051229	4.815526
245.226953	7999.848233	9.356109	-0.051211	4.815519
245.353333	7999.805462	9.361114	-0.051235	4.815506
245.373257	7999.833574	9.366119	-0.051239	4.815514
245.441618	7999.840050	9.371123	-0.051252	4.815516
245.348394	7999.807581	9.376128	-0.051235	4.815507
245.320614	7999.954521	9.381133	-0.051230	4.815550
245.403391	7999.832015	9.386138	-0.051245	4.815514
245.420452	7999.862216	9.391143	-0.051249	4.815523
245.233967	7999.858128	9.396147	-0.051214	4.815522
245.470423	7999.937827	9.401152	-0.051259	4.815544
245.295214	7999.848490	9.406157	-0.051226	4.815519
245.268051	7999.901464	9.411162	-0.051221	4.815535
245.350843	7999.819538	9.416167	-0.051237	4.815510
245.299748	7999.913770	9.421171	-0.051228	4.815538
245.260930	7999.823454	9.426176	-0.051221	4.815512
245.392123	7999.857652	9.431181	-0.051246	4.815521
245.664577	7999.921920	9.436186	-0.051297	4.815539
245.692663	7999.878614	9.441191	-0.051302	4.815526
245.481478	7999.858105	9.446195	-0.051263	4.815521
245.493585	7999.926670	9.451200	-0.051265	4.815541
245.450314	7999.888609	9.456205	-0.051258	4.815530
245.534929	7999.869719	9.461210	-0.051274	4.815524
245.833954	7999.850055	9.466215	-0.051329	4.815517
245.986987	7999.841893	9.471219	-0.051358	4.815514
245.615471	7999.962938	9.476224	-0.051289	4.815551
245.718910	7999.917658	9.481229	-0.051309	4.815537
245.738104	7999.847509	9.486234	-0.051313	4.815517
245.690002	7999.902278	9.491239	-0.051304	4.815533
245.625104	7999.845709	9.496243	-0.051292	4.815517
245.661053	7999.928546	9.501248	-0.051299	4.815541
245.613430	7999.809252	9.506253	-0.051290	4.815506
245.633848	7999.883292	9.511258	-0.051294	4.815528
245.815754	7999.971714	9.516263	-0.051329	4.815552
245.826018	7999.825597	9.521267	-0.051331	4.815510
245.789436	7999.882690	9.526272	-0.051324	4.815527
245.846343	7999.965870	9.531277	-0.051335	4.815551
245.829249	7999.791541	9.536282	-0.051332	4.815500
245.978743	7999.933898	9.541287	-0.051360	4.815541
245.882308	7999.920599	9.546291	-0.051342	4.815537
245.919207	7999.821905	9.551296	-0.051349	4.815508
245.918728	7999.930847	9.556301	-0.051350	4.815540
245.878185	7999.817007	9.561306	-0.051342	4.815507
245.973642	7999.941397	9.566311	-0.051360	4.815543
246.068208	7999.871409	9.571315	-0.051378	4.815522
245.936070	7999.871411	9.576320	-0.051354	4.815523
245.979018	7999.930869	9.581325	-0.051362	4.815540
245.992815	7999.875583	9.586330	-0.051365	4.815523
245.935398	7999.889619	9.591335	-0.051354	4.815528
246.034194	7999.951055	9.596339	-0.051373	4.815545
246.146236	7999.902712	9.601344	-0.051394	4.815531
246.111136	7999.918179	9.606349	-0.051388	4.815535
246.131074	7999.874741	9.611354	-0.051392	4.815523
246.333002	7999.886599	9.616359	-0.051430	4.815525
246.185599	7999.861789	9.621363	-0.051403	4.815518
246.248887	7999.910900	9.626368	-0.051415	4.815532
246.026741	7999.945743	9.631373	-0.051373	4.815544
246.103324	7999.863715	9.636378	-0.051388	4.815519
246.322052	7999.873712	9.641383	-0.051429	4.815521
246.092282	7999.863577	9.646387	-0.051386	4.815519
246.201688	7999.970041	9.651392	-0.051407	4.815550
246.406317	7999.883694	9.656397	-0.051445	4.815524
246.227800	7999.945947	9.661402	-0.051412	4.815543
246.326037	7999.897378	9.666407	-0.051431	4.815528
246.220415	7999.881793	9.671411	-0.051411	4.815524
246.327323	7999.855792	9.676416	-0.051432	4.815516
246.498358	7999.884234	9.681421	-0.051464	4.815523
246.463729	7999.922136	9.686426	-0.051457	4.815535
246.465835	7999.861319	9.691431	-0.051458	4.815517
246.255866	7999.837624	9.696435	-0.051419	4.815511
246.450332	7999.938000	9.701440	-0.051456	4.815539
246.539348	7999.859378	9.706445	-0.051472	4.815516
246.478522	7999.956658	9.711450	-0.051461	4.815545
246.585869	7999.895422	9.716455	-0.051482	4.815526
246.351092	7999.848895	9.721459	-0.051438	4.815514
246.364515	7999.863019	9.726464	-0.051441	4.815518
246.353276	7999.962175	9.731469	-0.051439	4.815547
246.206460	7999.896793	9.736474	-0.051412	4.815528
246.287767	7999.850083	9.741479	-0.051427	4.815514
246.187234	7999.862348	9.746483	-0.051409	4.815518
246.316073	7999.865539	9.751488	-0.051433	4.815519
246.422899	7999.922835	9.756493	-0.051453	4.815535
246.213788	7999.976046	9.761498	-0.051415	4.815552
246.375953	7999.941335	9.766503	-0.051445	4.815541
246.392924	7999.892508	9.771507	-0.051448	4.815526
246.463408	7999.899019	9.776512	-0.051462	4.815528
246.729320	7999.856389	9.781517	-0.051512	4.815514
246.709948	7999.846483	9.786522	-0.051508	4.815511
246.890762	7999.902852	9.791527	-0.051542	4.815527
246.779612	7999.984360	9.796531	-0.051522	4.815551
246.636651	7999.888068	9.801536	-0.051495	4.815524
246.703830	7999.910545	9.806541	-0.051508	4.815530
246.419455	7999.887771	9.811546	-0.051455	4.815525
246.491889	7999.898586	9.816551	-0.051469	4.815528
246.532343	7999.884316	9.821555	-0.051477	4.815523
246.520280	7999.859577	9.826560	-0.051475	4.815516
246.481842	7999.960426	9.831565	-0.051468	4.815546
246.480628	7999.852565	9.836570	-0.051468	4.815514
246.702126	7999.924549	9.841575	-0.051509	4.815534
246.681796	7999.971228	9.846579	-0.051506	4.815548
246.730327	7999.872722	9.851584	-0.051515	4.815519
246.870419	7999.909204	9.856589	-0.051541	4.815529
246.815218	7999.874150	9.861594	-0.051531	4.815519
247.074225	7999.910437	9.866599	-0.051580	4.815528
247.110215	7999.832016	9.871603	-0.051587	4.815505
246.863145	7999.974316	9.876608	-0.051541	4.815548
246.938538	7999.910422	9.881613	-0.051555	4.815529
247.079431	7999.852937	9.886618	-0.051582	4.815511
246.996013	7999.930626	9.891623	-0.051567	4.815534
246.872973	7999.876309	9.896627	-0.051544	4.815519
246.773989	7999.909958	9.901632	-0.051526	4.815529
246.819881	7999.906456	9.906637	-0.051534	4.815528
246.608742	7999.940410	9.911642	-0.051495	4.815539
246.711919	7999.887650	9.916647	-0.051515	4.815523
246.711761	7999.942134	9.921651	-0.051515	4.815539
246.827419	7999.916276	9.926656	-0.051537	4.815531
247.044433	7999.974304	9.931661	-0.051578	4.815547
246.900544	7999.955958	9.936666	-0.051551	4.815542
247.022546	7999.951563	9.941671	-0.051574	4.815540
246.914726	7999.897494	9.946675	-0.051554	4.815525
246.759505	7999.898187	9.951680	-0.051525	4.815526
246.897274	7999.887641	9.956685	-0.051551	4.815522
246.804911	7999.931009	9.961690	-0.051534	4.815535
246.684733	7999.844701	9.966695	-0.051512	4.815511
246.869349	7999.892588	9.971699	-0.051547	4.815524
246.909336	7999.899670	9.976704	-0.051555	4.815526
246.878442	7999.925886	9.981709	-0.051549	4.815533
246.934776	7999.910807	9.986714	-0.051560	4.815529
247.013920	8000.010372	9.991719	-0.051575	4.815557
246.894521	7999.873882	9.996723	-0.051553	4.815518
246.882132	7999.829915	10.001728	-0.051551	4.815505
246.989400	7999.895764	10.006733	-0.051571	4.815524
246.843888	7999.997003	10.011738	-0.051544	4.815554
246.779386	7999.916943	10.016743	-0.051532	4.815531
246.776425	7999.874197	10.021747	-0.051532	4.815519
247.025811	7999.897512	10.026752	-0.051579	4.815524
246.934005	7999.961180	10.031757	-0.051562	4.815543
247.072642	7999.934629	10.036762	-0.051588	4.815535
247.334299	7999.954940	10.041767	-0.051637	4.815540
247.085956	7999.922073	10.046771	-0.051591	4.815531
247.035515	7999.934087	10.051776	-0.051582	4.815535
247.154575	7999.946731	10.056781	-0.051604	4.815538
247.053533	7999.917336	10.061786	-0.051585	4.815530
247.162200	7999.957578	10.066791	-0.051606	4.815541
247.147267	7999.937064	10.071795	-0.051603	4.815535
247.111624	7999.890581	10.076800	-0.051597	4.815522
247.132468	7999.955020	10.081805	-0.051601	4.815541
247.202821	7999.969005	10.086810	-0.051615	4.815544
247.344572	7999.988428	10.091815	-0.051641	4.815549
246.994225	7999.951760	10.096819	-0.051576	4.815540
246.960565	7999.944824	10.101824	-0.051570	4.815538
247.172059	7999.970724	10.106829	-0.051610	4.815545
247.261520	7999.929487	10.111834	-0.051627	4.815532
247.151841	7999.950145	10.116839	-0.051606	4.815539
247.138607	7999.938203	10.121843	-0.051604	4.815536
247.097137	7999.932208	10.126848	-0.051597	4.815534
247.315670	7999.982786	10.131853	-0.051638	4.815548
247.130955	7999.929598	10.136858	-0.051604	4.815533
247.101977	7999.917399	10.141863	-0.051598	4.815530
247.199324	7999.995903	10.146867	-0.051617	4.815552
247.232361	7999.952677	10.151872	-0.051623	4.815539
247.064012	7999.984125	10.156877	-0.051592	4.815549
246.964377	7999.949413	10.161882	-0.051574	4.815540
246.971591	7999.933533	10.166887	-0.051575	4.815535
247.054889	7999.924234	10.171891	-0.051591	4.815532
247.102682	7999.901540	10.176896	-0.051600	4.815525
247.130798	7999.931923	10.181901	-0.051606	4.815534
247.089923	7999.913122	10.186906	-0.051598	4.815528
247.322805	7999.973546	10.191911	-0.051642	4.815545
247.140388	7999.892629	10.196915	-0.051608	4.815522
247.147172	7999.924800	10.201920	-0.051610	4.815532
247.323139	7999.928761	10.206925	-0.051643	4.815532
247.422993	7999.927208	10.211930	-0.051662	4.815531
247.426858	7999.947584	10.216935	-0.051663	4.815537
247.377391	7999.936118	10.221939	-0.051654	4.815534
247.489677	7999.900593	10.226944	-0.051675	4.815523
247.293451	7999.932655	10.231949	-0.051638	4.815533
247.043962	7999.890157	10.236954	-0.051592	4.815522
247.187052	7999.886106	10.241959	-0.051619	4.815520
247.123913	7999.903252	10.246963	-0.051608	4.815525
247.103393	7999.884783	10.251968	-0.051604	4.815520
247.284629	7999.910190	10.256973	-0.051638	4.815527
247.373892	7999.865745	10.261978	-0.051655	4.815513
247.590379	7999.977166	10.266983	-0.051695	4.815545
247.227986	8000.021466	10.271987	-0.051628	4.815559
247.262647	7999.925936	10.276992	-0.051635	4.815531
247.312488	7999.917159	10.281997	-0.051644	4.815528
247.200267	7999.892921	10.287002	-0.051624	4.815522
247.362889	7999.952199	10.292007	-0.051654	4.815538
247.353401	7999.962745	10.297011	-0.051653	4.815542
247.337035	7999.940072	10.302016	-0.051650	4.815535
247.260266	7999.951655	10.307021	-0.051636	4.815539
247.353309	7999.890185	10.312026	-0.051653	4.815520
247.402554	7999.916642	10.317031	-0.051663	4.815528
247.230601	7999.914924	10.322035	-0.051631	4.815528
247.147317	7999.924266	10.327040	-0.051616	4.815531
247.261284	7999.984885	10.332045	-0.051637	4.815548
247.372010	7999.923704	10.337050	-0.051658	4.815530
247.242428	7999.971805	10.342055	-0.051634	4.815545
247.455958	7999.932593	10.347059	-0.051674	4.815532
247.319116	7999.936788	10.352064	-0.051649	4.815534
247.308288	7999.948380	10.357069	-0.051647	4.815537
247.576569	7999.947441	10.362074	-0.051697	4.815536
247.643823	7999.993415	10.367079	-0.051710	4.815549
247.344322	7999.966120	10.372083	-0.051655	4.815542
247.313102	7999.943204	10.377088	-0.051649	4.815536
247.538772	7999.990696	10.382093	-0.051691	4.815549
247.281514	7999.959818	10.387098	-0.051644	4.815541
247.372585	7999.982686	10.392103	-0.051661	4.815547
247.526828	8000.055712	10.397107	-0.051690	4.815568
247.508365	7999.973197	10.402112	-0.051687	4.815544
247.615742	7999.955748	10.407117	-0.051707	4.815538
247.435072	7999.876994	10.412122	-0.051674	4.815516
247.464019	7999.954382	10.417127	-0.051679	4.815538
247.410191	7999.961000	10.422131	-0.051669	4.815541
247.514914	7999.960595	10.427136	-0.051689	4.815540
247.739596	7999.976032	10.432141	-0.051731	4.815543
247.498368	7999.953959	10.437146	-0.051687	4.815538
247.459480	7999.996065	10.442151	-0.051680	4.815551
247.492299	7999.947495	10.447155	-0.051686	4.815536
247.629300	7999.901694	10.452160	-0.051712	4.815522
247.544665	7999.922761	10.457165	-0.051696	4.815529
247.307853	7999.933868	10.462170	-0.051652	4.815533
247.610238	7999.956981	10.467175	-0.051709	4.815538
247.516674	7999.946931	10.472179	-0.051692	4.815536
247.494046	7999.931632	10.477184	-0.051688	4.815532
247.434219	7999.960579	10.482189	-0.051677	4.815540
247.537393	7999.953741	10.487194	-0.051696	4.815538
247.444618	7999.927685	10.492199	-0.051679	4.815531
247.822338	7999.946688	10.497203	-0.051750	4.815534
247.668472	7999.957013	10.502208	-0.051721	4.815538
247.542996	7999.962462	10.507213	-0.051698	4.815540
247.481728	7999.931579	10.512218	-0.051687	4.815532
247.650402	7999.998433	10.517223	-0.051719	4.815550
247.690388	7999.983087	10.522227	-0.051726	4.815546
247.626044	7999.940407	10.527232	-0.051715	4.815533
247.611044	7999.991446	10.532237	-0.051712	4.815548
247.610594	7999.912430	10.537242	-0.051712	4.815525
247.770761	7999.939630	10.542247	-0.051742	4.815532
247.700807	7999.920353	10.547251	-0.051730	4.815527
247.699818	7999.912882	10.552256	-0.051730	4.815525
247.589113	7999.927116	10.557261	-0.051709	4.815530
247.581777	7999.884299	10.562266	-0.051708	4.815517
247.695067	7999.943840	10.567271	-0.051729	4.815534
247.583262	7999.973007	10.572275	-0.051709	4.815543
247.719110	7999.964567	10.577280	-0.051734	4.815540
247.724184	7999.953991	10.582285	-0.051736	4.815537
247.690486	7999.838121	10.587290	-0.051730	4.815503
247.904027	7999.922795	10.592295	-0.051770	4.815527
247.869132	7999.961761	10.597299	-0.051763	4.815538
247.797337	7999.929639	10.602304	-0.051750	4.815529
247.714424	7999.967822	10.607309	-0.051735	4.815541
247.669319	7999.892348	10.612314	-0.051727	4.815519
247.932859	7999.958615	10.617319	-0.051776	4.815537
247.900247	7999.936744	10.622323	-0.051770	4.815531
247.738315	7999.871111	10.627328	-0.051740	4.815513
247.873292	7999.961978	10.632333	-0.051766	4.815538
247.789499	7999.914708	10.637338	-0.051750	4.815525
247.649124	7999.910302	10.642343	-0.051725	4.815524
247.716491	8000.028901	10.647347	-0.051737	4.815559
247.702767	7999.977435	10.652352	-0.051735	4.815544
247.870242	7999.937471	10.657357	-0.051766	4.815531
247.621450	7999.905663	10.662362	-0.051720	4.815523
247.899764	7999.904888	10.667367	-0.051772	4.815522
247.841307	7999.924247	10.672371	-0.051762	4.815528
247.698750	7999.884561	10.677376	-0.051735	4.815517
247.862375	7999.956673	10.682381	-0.051766	4.815537
247.913417	7999.941508	10.687386	-0.051776	4.815532
248.050774	7999.973676	10.692391	-0.051802	4.815541
247.794725	7999.956700	10.697395	-0.051754	4.815537
247.888966	7999.927289	10.702400	-0.051772	4.815528
247.849917	7999.970460	10.707405	-0.051765	4.815541
247.736379	7999.948335	10.712410	-0.051744	4.815535
248.101895	7999.988501	10.717415	-0.051813	4.815545
247.808707	7999.953831	10.722419	-0.051758	4.815536
247.823477	7999.934870	10.727424	-0.051761	4.815531
248.074633	7999.976372	10.732429	-0.051808	4.815542
247.942424	7999.914427	10.737434	-0.051784	4.815524
247.975057	7999.926729	10.742439	-0.051790	4.815528
248.051981	7999.926938	10.747443	-0.051805	4.815527
247.957578	7999.916874	10.752448	-0.051787	4.815525
247.934341	7999.970983	10.757453	-0.051783	4.815541
247.825650	7999.933986	10.762458	-0.051763	4.815530
248.062263	7999.991270	10.767463	-0.051808	4.815546
247.997589	7999.975284	10.772467	-0.051796	4.815542
247.883756	7999.962766	10.777472	-0.051775	4.815538
248.014881	7999.978813	10.782477	-0.051799	4.815542
247.965391	7999.891519	10.787482	-0.051790	4.815517
247.871920	7999.877198	10.792487	-0.051773	4.815513
247.757888	7999.883902	10.797491	-0.051752	4.815516
247.851956	7999.896138	10.802496	-0.051770	4.815519
247.844400	7999.976135	10.807501	-0.051769	4.815542
247.845926	7999.908898	10.812506	-0.051769	4.815523
247.842576	7999.962264	10.817511	-0.051769	4.815538
247.989225	7999.981768	10.822515	-0.051797	4.815543
247.646988	7999.911054	10.827520	-0.051733	4.815524
247.803742	7999.977714	10.832525	-0.051763	4.815543
247.984926	7999.913410	10.837530	-0.051797	4.815523
248.114345	7999.937972	10.842535	-0.051821	4.815530
248.141806	7999.945918	10.847539	-0.051826	4.815532
248.028844	7999.916327	10.852544	-0.051805	4.815524
247.990413	7999.977664	10.857549	-0.051799	4.815542
248.095656	7999.926004	10.862554	-0.051818	4.815527
248.151278	7999.919458	10.867559	-0.051829	4.815524
248.110066	7999.951914	10.872563	-0.051822	4.815534
247.932170	7999.896699	10.877568	-0.051789	4.815519
247.947270	7999.970658	10.882573	-0.051792	4.815540
248.025737	7999.964485	10.887578	-0.051807	4.815538
247.978510	7999.986163	10.892583	-0.051798	4.815545
247.837380	7999.950772	10.897587	-0.051772	4.815535
247.862906	7999.920238	10.902592	-0.051777	4.815526
248.094377	7999.964623	10.907597	-0.051820	4.815538
247.996617	7999.970524	10.912602	-0.051802	4.815540
248.114401	7999.951108	10.917607	-0.051825	4.815534
248.078398	7999.962290	10.922611	-0.051818	4.815537
247.925557	7999.934183	10.927616	-0.051790	4.815530
248.140767	7999.961215	10.932621	-0.051830	4.815537
248.338545	7999.931358	10.937626	-0.051867	4.815527
248.406439	7999.944236	10.942631	-0.051880	4.815530
248.148183	8000.004120	10.947635	-0.051832	4.815549
248.071567	7999.949490	10.952640	-0.051818	4.815533
248.179321	7999.958747	10.957645	-0.051839	4.815536
248.093414	7999.969113	10.962650	-0.051823	4.815539
248.144309	7999.920838	10.967655	-0.051833	4.815525
248.042306	7999.964049	10.972659	-0.051814	4.815538
248.178383	7999.957749	10.977664	-0.051839	4.815535
248.315290	7999.983502	10.982669	-0.051865	4.815542
248.157678	7999.971337	10.987674	-0.051836	4.815539
247.936408	7999.958133	10.992679	-0.051795	4.815537
247.877247	7999.983888	10.997683	-0.051784	4.815544
248.047922	7999.920481	11.002688	-0.051816	4.815525
248.112212	7999.930096	11.007693	-0.051828	4.815528
248.084323	7999.928594	11.012698	-0.051824	4.815527
247.909892	7999.923631	11.017703	-0.051791	4.815527
248.148275	7999.961720	11.022707	-0.051836	4.815537
248.161448	7999.890401	11.027712	-0.051839	4.815516
248.181783	7999.972990	11.032717	-0.051843	4.815540
247.963009	7999.912835	11.037722	-0.051802	4.815523
248.029020	7999.954518	11.042727	-0.051815	4.815535
247.955523	7999.959747	11.047731	-0.051801	4.815537
248.002235	7999.961599	11.052736	-0.051810	4.815537
248.062374	7999.981827	11.057741	-0.051822	4.815543
248.096643	7999.931144	11.062746	-0.051828	4.815528
247.902037	7999.979251	11.067751	-0.051792	4.815543
247.896392	7999.947140	11.072755	-0.051791	4.815533
248.237418	7999.985838	11.077760	-0.051855	4.815543
248.092452	8000.035824	11.082765	-0.051829	4.815558
248.081272	7999.953427	11.087770	-0.051827	4.815534
248.218745	7999.997345	11.092775	-0.051852	4.815547
248.049771	7999.960431	11.097779	-0.051821	4.815537
248.086146	7999.929007	11.102784	-0.051828	4.815527
248.376916	8000.022421	11.107789	-0.051883	4.815553
248.091384	7999.978262	11.112794	-0.051830	4.815542
248.067533	7999.998186	11.117799	-0.051826	4.815547
248.242037	7999.978629	11.122803	-0.051858	4.815541
248.192131	7999.897736	11.127808	-0.051849	4.815518
248.153962	7999.959078	11.132813	-0.051842	4.815536
248.091069	7999.920692	11.137818	-0.051831	4.815525
248.279151	7999.981457	11.142823	-0.051866	4.815542
248.165250	8000.010590	11.147827	-0.051845	4.815551
248.080285	7999.931260	11.152832	-0.051830	4.815528
248.167666	8000.020284	11.157837	-0.051846	4.815553
248.213195	7999.963377	11.162842	-0.051855	4.815537
248.186171	7999.961889	11.167847	-0.051850	4.815536
248.352756	7999.966766	11.172851	-0.051881	4.815537
248.324904	7999.924681	11.177856	-0.051876	4.815525
248.257663	7999.998364	11.182861	-0.051864	4.815547
248.210909	7999.952766	11.187866	-0.051856	4.815533
248.484616	7999.965801	11.192871	-0.051907	4.815536
248.297944	8000.000154	11.197875	-0.051872	4.815547
248.252323	7999.974866	11.202880	-0.051864	4.815540
248.273026	7999.960273	11.207885	-0.051868	4.815535
248.072046	7999.928176	11.212890	-0.051831	4.815527
248.143305	7999.960333	11.217895	-0.051844	4.815536
248.124779	7999.970732	11.222899	-0.051841	4.815539
248.154107	7999.909289	11.227904	-0.051847	4.815521
248.205868	7999.950739	11.232909	-0.051857	4.815533
248.256696	7999.914210	11.237914	-0.051867	4.815522
248.425347	7999.920190	11.242919	-0.051898	4.815523
248.450679	7999.937713	11.247923	-0.051903	4.815528
248.146787	7999.937043	11.252928	-0.051847	4.815529
248.384792	7999.963379	11.257933	-0.051891	4.815536
248.449572	7999.945235	11.262938	-0.051904	4.815530
248.339567	7999.946663	11.267943	-0.051883	4.815531
248.265112	8000.008481	11.272947	-0.051870	4.815549
248.404530	7999.908251	11.277952	-0.051896	4.815519
248.608782	7999.974621	11.282957	-0.051934	4.815538
248.301167	7999.945053	11.287962	-0.051877	4.815531
248.149786	7999.956486	11.292967	-0.051849	4.815535
248.252758	7999.992365	11.297971	-0.051869	4.815545
248.031543	7999.933238	11.302976	-0.051828	4.815528
248.252853	7999.939009	11.307981	-0.051869	4.815529
248.247407	7999.947486	11.312986	-0.051868	4.815532
248.131901	7999.926397	11.317991	-0.051847	4.815526
248.167431	7999.979330	11.322995	-0.051854	4.815541
248.191216	7999.914592	11.328000	-0.051859	4.815522
248.480635	7999.967400	11.333005	-0.051913	4.815536
248.333157	7999.941517	11.338010	-0.051886	4.815529
248.481116	7999.938614	11.343015	-0.051913	4.815528
248.554848	7999.937704	11.348019	-0.051927	4.815527
248.106529	7999.890888	11.353024	-0.051844	4.815516
248.253130	7999.924275	11.358029	-0.051872	4.815525
248.192203	7999.945729	11.363034	-0.051861	4.815531
248.304646	7999.947587	11.368039	-0.051882	4.815531
248.266990	7999.974761	11.373043	-0.051875	4.815539
248.301950	7999.943313	11.378048	-0.051882	4.815530
248.349901	7999.987906	11.383053	-0.051891	4.815543
248.172633	7999.917748	11.388058	-0.051858	4.815523
248.388424	7999.973625	11.393063	-0.051899	4.815538
248.418545	7999.917535	11.398067	-0.051904	4.815522
248.346125	7999.869381	11.403072	-0.051891	4.815508
248.468628	7999.893831	11.408077	-0.051914	4.815515
248.513473	7999.882837	11.413082	-0.051923	4.815511
248.539923	7999.932418	11.418087	-0.051928	4.815526
248.336852	7999.959027	11.423091	-0.051890	4.815534
248.287635	7999.883484	11.428096	-0.051882	4.815513
248.561504	7999.955263	11.433101	-0.051933	4.815532
248.453134	7999.938562	11.438106	-0.051913	4.815528
248.344480	7999.890885	11.443111	-0.051893	4.815514
248.566254	7999.966084	11.448115	-0.051934	4.815535
248.500956	7999.904163	11.453120	-0.051922	4.815518
248.427334	7999.922206	11.458125	-0.051909	4.815523
248.289329	7999.966965	11.463130	-0.051884	4.815537
248.322534	7999.913060	11.468135	-0.051890	4.815521
248.275503	7999.916586	11.473139	-0.051881	4.815522
248.275210	7999.889902	11.478144	-0.051882	4.815514
248.419730	8000.008696	11.483149	-0.051909	4.815548
248.306289	7999.951328	11.488154	-0.051888	4.815532
248.438440	7999.869136	11.493159	-0.051913	4.815508
248.446803	7999.921626	11.498163	-0.051915	4.815523
248.255416	7999.903569	11.503168	-0.051879	4.815518
248.586038	7999.928214	11.508173	-0.051941	4.815524
248.562164	7999.917166	11.513178	-0.051937	4.815521
248.435667	7999.937549	11.518183	-0.051913	4.815528
248.612798	7999.975708	11.523187	-0.051947	4.815538
248.523338	7999.937956	11.528192	-0.051930	4.815527
248.667832	7999.892277	11.533197	-0.051957	4.815513
248.521990	7999.915548	11.538202	-0.051931	4.815521
248.546887	7999.892480	11.543207	-0.051935	4.815514
248.516741	7999.914437	11.548211	-0.051930	4.815520
248.442607	7999.839555	11.553216	-0.051916	4.815499
248.443463	7999.896195	11.558221	-0.051917	4.815515
248.430641	7999.863966	11.563226	-0.051915	4.815506
248.533287	7999.828284	11.568231	-0.051934	4.815495
248.649521	7999.892148	11.573235	-0.051956	4.815513
248.320095	7999.821641	11.578240	-0.051895	4.815494
248.504359	7999.895160	11.583245	-0.051929	4.815515
248.339364	7999.941614	11.588250	-0.051899	4.815529
248.431864	7999.877998	11.593255	-0.051916	4.815510
248.555987	7999.911019	11.598259	-0.051940	4.815519
248.498263	7999.848153	11.603264	-0.051929	4.815501
248.530553	7999.951230	11.608269	-0.051936	4.815531
248.627865	7999.904780	11.613274	-0.051954	4.815517
248.562043	7999.902659	11.618279	-0.051942	4.815517
248.633653	7999.916666	11.623283	-0.051955	4.815520
248.489450	7999.860932	11.628288	-0.051929	4.815505
248.633985	7999.930598	11.633293	-0.051956	4.815524
248.445520	7999.938221	11.638298	-0.051921	4.815528
248.266131	7999.950264	11.643303	-0.051888	4.815532
248.445908	7999.906230	11.648307	-0.051922	4.815518
248.544826	7999.835242	11.653312	-0.051940	4.815497
248.530264	7999.940758	11.658317	-0.051938	4.815528
248.259885	7999.856264	11.663322	-0.051888	4.815504
248.526441	7999.861706	11.668327	-0.051938	4.815505
248.733433	7999.908896	11.673331	-0.051976	4.815518
248.492395	7999.862260	11.678336	-0.051932	4.815505
248.510668	7999.897824	11.683341	-0.051935	4.815515
248.545446	7999.896278	11.688346	-0.051942	4.815515
248.425149	7999.903946	11.693351	-0.051920	4.815518
248.535310	7999.944215	11.698355	-0.051941	4.815529
248.627926	7999.899825	11.703360	-0.051958	4.815515
248.563114	7999.930827	11.708365	-0.051946	4.815525
248.374994	7999.944864	11.713370	-0.051912	4.815530
248.460126	7999.958024	11.718375	-0.051928	4.815533
248.512822	7999.926866	11.723379	-0.051938	4.815524
248.502817	7999.935268	11.728384	-0.051936	4.815526
248.657895	7999.957046	11.733389	-0.051965	4.815532
248.586537	7999.934542	11.738394	-0.051952	4.815526
248.487250	7999.942553	11.743399	-0.051934	4.815528
248.619978	7999.972511	11.748403	-0.051959	4.815537
248.519740	7999.863026	11.753408	-0.051940	4.815505
248.492757	7999.887171	11.758413	-0.051936	4.815512
248.513695	7999.909962	11.763418	-0.051940	4.815519
248.624963	7999.880829	11.768423	-0.051961	4.815510
248.687274	7999.969445	11.773427	-0.051973	4.815535
248.547962	7999.900974	11.778432	-0.051947	4.815516
248.683683	7999.958748	11.783437	-0.051973	4.815532
248.701571	7999.909933	11.788442	-0.051976	4.815518
248.658278	7999.908180	11.793447	-0.051968	4.815518
248.659774	7999.961626	11.798451	-0.051969	4.815533
248.390384	7999.886759	11.803456	-0.051919	4.815513
248.601556	7999.914793	11.808461	-0.051958	4.815520
248.443105	7999.887662	11.813466	-0.051929	4.815513
248.615075	7999.910784	11.818471	-0.051961	4.815518
248.667435	7999.945837	11.823475	-0.051971	4.815528
248.571336	7999.873800	11.828480	-0.051954	4.815508
248.686295	7999.905603	11.833485	-0.051975	4.815517
248.514248	7999.900679	11.838490	-0.051944	4.815516
248.492040	7999.870433	11.843495	-0.051940	4.815507
248.770216	7999.939079	11.848499	-0.051992	4.815526
248.908650	7999.865532	11.853504	-0.052018	4.815504
248.812503	7999.897091	11.858509	-0.052000	4.815513
248.682046	7999.978287	11.863514	-0.051976	4.815538
248.638630	7999.966919	11.868519	-0.051968	4.815535
248.637057	7999.886813	11.873523	-0.051968	4.815511
248.534529	7999.847780	11.878528	-0.051949	4.815500
248.575568	7999.936048	11.883533	-0.051957	4.815526
248.603044	7999.894866	11.888538	-0.051963	4.815514
248.589713	7999.903213	11.893543	-0.051960	4.815516
248.539541	7999.950475	11.898547	-0.051951	4.815530
248.589105	7999.886158	11.903552	-0.051961	4.815511
248.629215	7999.880426	11.908557	-0.051968	4.815509
248.453261	7999.906410	11.913562	-0.051936	4.815518
248.619120	7999.901664	11.918567	-0.051967	4.815516
248.797400	7999.933434	11.923571	-0.052000	4.815524
248.514006	7999.885038	11.928576	-0.051948	4.815511
248.592277	7999.926922	11.933581	-0.051963	4.815523
248.682802	7999.918810	11.938586	-0.051980	4.815520
248.652015	7999.846771	11.943591	-0.051974	4.815499
248.680435	7999.925221	11.948595	-0.051980	4.815522
248.649271	7999.893761	11.953600	-0.051974	4.815513
248.592498	7999.911012	11.958605	-0.051964	4.815518
248.623567	7999.913676	11.963610	-0.051970	4.815519
248.741624	7999.913490	11.968615	-0.051992	4.815518
248.632487	7999.936293	11.973619	-0.051972	4.815526
248.371689	7999.906422	11.978624	-0.051924	4.815518
248.505180	7999.935324	11.983629	-0.051949	4.815526
248.444036	7999.921530	11.988634	-0.051938	4.815522
248.707478	7999.888474	11.993639	-0.051987	4.815511
248.602798	7999.932710	11.998643	-0.051968	4.815525
248.683877	7999.928716	12.003648	-0.051983	4.815523
248.832263	7999.983494	12.008653	-0.052011	4.815538
248.788636	7999.957170	12.013658	-0.052003	4.815531
248.913153	7999.937865	12.018663	-0.052027	4.815525
248.850684	7999.965703	12.023667	-0.052015	4.815533
248.575201	7999.954815	12.028672	-0.051964	4.815531
248.814845	7999.954479	12.033677	-0.052009	4.815530
248.785306	7999.990331	12.038682	-0.052004	4.815541
248.849573	7999.931593	12.043687	-0.052016	4.815523
248.589367	7999.972220	12.048691	-0.051968	4.815536
248.720481	7999.969043	12.053696	-0.051992	4.815535
248.861984	7999.999145	12.058701	-0.052019	4.815543
248.601482	7999.982094	12.063706	-0.051971	4.815539
248.502158	7999.948453	12.068711	-0.051953	4.815530
248.809925	7999.983406	12.073715	-0.052010	4.815538
248.577206	7999.940109	12.078720	-0.051967	4.815527
248.625254	7999.949459	12.083725	-0.051976	4.815529
248.551835	7999.947213	12.088730	-0.051963	4.815529
248.780974	7999.879421	12.093735	-0.052006	4.815508
248.741978	7999.937546	12.098739	-0.051999	4.815525
248.629136	7999.941064	12.103744	-0.051978	4.815527
248.929965	8000.012217	12.108749	-0.052034	4.815546
248.837459	7999.976550	12.113754	-0.052017	4.815536
248.784631	7999.997069	12.118759	-0.052008	4.815542
248.786651	7999.975762	12.123763	-0.052008	4.815536
248.627957	7999.928335	12.128768	-0.051979	4.815523
248.520381	7999.999224	12.133773	-0.051959	4.815544
248.541592	7999.988911	12.138778	-0.051963	4.815541
248.704988	7999.946745	12.143783	-0.051994	4.815528
248.526351	7999.968413	12.148787	-0.051961	4.815535
248.382174	7999.905202	12.153792	-0.051934	4.815518
248.756755	7999.945519	12.158797	-0.052004	4.815528
248.835954	7999.946834	12.163802	-0.052019	4.815528
248.698162	7999.915768	12.168807	-0.051994	4.815519
248.877756	7999.998824	12.173811	-0.052028	4.815542
248.767470	7999.990636	12.178816	-0.052007	4.815541
248.847500	7999.986624	12.183821	-0.052022	4.815539
248.803785	7999.978455	12.188826	-0.052015	4.815537
248.687028	7999.947733	12.193831	-0.051993	4.815528
248.621547	7999.990473	12.198835	-0.051981	4.815541
248.568202	7999.993895	12.203840	-0.051971	4.815542
248.782805	7999.999558	12.208845	-0.052012	4.815543
248.674424	8000.001013	12.213850	-0.051992	4.815544
248.597248	8000.031814	12.218855	-0.051978	4.815553
248.585769	8000.027375	12.223859	-0.051976	4.815552
248.526908	7999.960218	12.228864	-0.051965	4.815533
248.726250	7999.969904	12.233869	-0.052002	4.815535
248.843670	7999.904558	12.238874	-0.052024	4.815515
248.648848	7999.939846	12.243879	-0.051988	4.815526
248.773316	7999.994233	12.248883	-0.052012	4.815542
248.691532	7999.964082	12.253888	-0.051997	4.815533
248.826569	7999.993010	12.258893	-0.052022	4.815541
248.890346	7999.969509	12.263898	-0.052034	4.815534
248.707035	8000.016732	12.268903	-0.052000	4.815548
248.961323	7999.949350	12.273907	-0.052048	4.815528
248.899145	7999.901363	12.278912	-0.052037	4.815514
248.960206	7999.957919	12.283917	-0.052048	4.815530
248.848812	7999.944372	12.288922	-0.052028	4.815527
248.761003	7999.846837	12.293927	-0.052012	4.815498
248.983822	7999.960505	12.298931	-0.052053	4.815531
248.607825	7999.924479	12.303936	-0.051984	4.815522
248.681153	7999.979099	12.308941	-0.051998	4.815537
248.765862	7999.940987	12.313946	-0.052014	4.815526
248.643930	7999.974261	12.318951	-0.051991	4.815536
248.692202	7999.956915	12.323955	-0.052000	4.815531
248.659077	7999.931831	12.328960	-0.051994	4.815524
248.650679	7999.997932	12.333965	-0.051993	4.815543
248.822424	7999.950562	12.338970	-0.052025	4.815528
248.739959	7999.927876	12.343975	-0.052010	4.815522
248.626418	7999.951674	12.348979	-0.051989	4.815530
248.704439	7999.893161	12.353984	-0.052004	4.815512
248.787808	7999.930857	12.358989	-0.052020	4.815523
248.839448	7999.939198	12.363994	-0.052030	4.815525
248.596461	7999.925638	12.368999	-0.051985	4.815522
248.648809	7999.978847	12.374003	-0.051995	4.815537
248.826681	7999.962550	12.379008	-0.052028	4.815532
248.782014	7999.949025	12.384013	-0.052020	4.815528
248.553472	7999.977353	12.389018	-0.051978	4.815537
248.766673	7999.994742	12.394023	-0.052018	4.815542
248.986396	7999.952428	12.399027	-0.052059	4.815528
248.822732	7999.925211	12.404032	-0.052028	4.815521
248.785577	7999.921421	12.409037	-0.052022	4.815520
248.697147	7999.956311	12.414042	-0.052006	4.815531
248.761478	7999.939227	12.419047	-0.052018	4.815525
248.829443	7999.976671	12.424051	-0.052031	4.815536
249.001248	7999.934642	12.429056	-0.052063	4.815523
248.650992	7999.947098	12.434061	-0.051998	4.815528
248.775172	7999.934195	12.439066	-0.052021	4.815524
248.707789	7999.921368	12.444071	-0.052009	4.815520
248.819731	8000.006523	12.449075	-0.052030	4.815545
248.685236	7999.939198	12.454080	-0.052005	4.815526
248.833644	7999.957664	12.459085	-0.052033	4.815530
248.766194	7999.934155	12.464090	-0.052021	4.815524
248.884221	7999.927561	12.469095	-0.052043	4.815521
248.864528	7999.979593	12.474099	-0.052040	4.815537
248.851121	7999.942015	12.479104	-0.052037	4.815526
248.991727	7999.974238	12.484109	-0.052064	4.815534
248.870300	8000.005384	12.489114	-0.052042	4.815544
248.829200	7999.953469	12.494119	-0.052034	4.815529
249.057665	7999.965767	12.499123	-0.052077	4.815532
248.814663	7999.919097	12.504128	-0.052032	4.815519
248.972685	7999.967625	12.509133	-0.052062	4.815532
248.901863	7999.979305	12.514138	-0.052049	4.815536
248.965068	7999.902394	12.519143	-0.052061	4.815513
248.941018	7999.971444	12.524147	-0.052056	4.815534
248.795580	7999.946660	12.529152	-0.052030	4.815527
248.807592	7999.907361	12.534157	-0.052032	4.815516
248.882982	7999.949199	12.539162	-0.052046	4.815528
248.771072	7999.873699	12.544167	-0.052026	4.815506
248.917258	7999.958346	12.549171	-0.052053	4.815530
248.873635	7999.945906	12.554176	-0.052045	4.815527
249.107860	7999.966843	12.559181	-0.052089	4.815532
248.919561	7999.964855	12.564186	-0.052054	4.815532
248.795185	7999.932940	12.569191	-0.052031	4.815523
248.874362	7999.948139	12.574195	-0.052046	4.815527
248.970099	7999.932636	12.579200	-0.052064	4.815522
249.068771	7999.887276	12.584205	-0.052083	4.815508
249.072411	7999.889493	12.589210	-0.052084	4.815509
248.991777	7999.927714	12.594215	-0.052069	4.815521
249.167111	7999.925260	12.599219	-0.052102	4.815519
249.161018	7999.924114	12.604224	-0.052101	4.815519
249.103347	8000.003295	12.609229	-0.052091	4.815542
249.030762	8000.017082	12.614234	-0.052077	4.815547
248.940154	7999.896004	12.619239	-0.052061	4.815512
248.808884	7999.939806	12.624243	-0.052037	4.815525
248.848912	7999.875332	12.629248	-0.052044	4.815506
248.840989	7999.947849	12.634253	-0.052043	4.815527
248.743993	7999.945218	12.639258	-0.052025	4.815527
248.860302	7999.920439	12.644263	-0.052047	4.815519
249.102996	7999.961806	12.649267	-0.052093	4.815530
248.871853	7999.902514	12.654272	-0.052050	4.815514
249.056993	7999.927988	12.659277	-0.052084	4.815520
248.913714	7999.937417	12.664282	-0.052058	4.815524
248.973910	7999.889293	12.669287	-0.052069	4.815509
249.093565	7999.926514	12.674291	-0.052092	4.815520
248.905231	7999.889281	12.679296	-0.052057	4.815510
249.205716	7999.901688	12.684301	-0.052113	4.815512
249.049402	7999.915176	12.689306	-0.052085	4.815517
248.881210	7999.916721	12.694311	-0.052053	4.815518
249.054831	7999.969776	12.699315	-0.052086	4.815532
248.781485	7999.954651	12.704320	-0.052035	4.815529
248.760119	7999.885970	12.709325	-0.052032	4.815509
248.885747	7999.915812	12.714330	-0.052055	4.815518
248.990623	7999.886574	12.719335	-0.052075	4.815508
248.900112	7999.954539	12.724339	-0.052058	4.815529
248.732613	7999.945415	12.729344	-0.052027	4.815527
249.080008	7999.960725	12.734349	-0.052092	4.815530
249.153909	7999.949137	12.739354	-0.052106	4.815526
249.065467	7999.949849	12.744359	-0.052090	4.815527
249.089426	7999.985507	12.749363	-0.052095	4.815537
249.002679	7999.943526	12.754368	-0.052079	4.815525
249.161735	7999.936534	12.759373	-0.052109	4.815522
249.189562	7999.959438	12.764378	-0.052114	4.815529
248.989672	7999.900656	12.769383	-0.052077	4.815513
248.925661	7999.979733	12.774387	-0.052066	4.815536
248.877103	7999.955465	12.779392	-0.052057	4.815529
249.089899	7999.938670	12.784397	-0.052097	4.815523
248.959771	7999.940838	12.789402	-0.052073	4.815524
249.064950	7999.869952	12.794407	-0.052092	4.815503
249.069096	7999.929850	12.799411	-0.052094	4.815521
249.093530	7999.971924	12.804416	-0.052098	4.815533
248.969929	8000.003034	12.809421	-0.052076	4.815542
248.998411	7999.981093	12.814426	-0.052081	4.815536
249.051878	7999.901885	12.819431	-0.052091	4.815513
249.150808	7999.947312	12.824435	-0.052110	4.815525
248.765485	7999.926086	12.829440	-0.052038	4.815521
248.857229	7999.898769	12.834445	-0.052056	4.815513
249.195897	7999.885099	12.839450	-0.052119	4.815507
249.051436	7999.888100	12.844455	-0.052092	4.815508
249.089702	7999.945352	12.849459	-0.052100	4.815525
249.132199	7999.878782	12.854464	-0.052108	4.815505
248.948638	7999.922797	12.859469	-0.052074	4.815519
249.287875	7999.948654	12.864474	-0.052137	4.815525
249.245251	7999.897782	12.869479	-0.052130	4.815510
249.219552	7999.989234	12.874483	-0.052125	4.815537
249.209263	7999.974135	12.879488	-0.052124	4.815533
249.203158	7999.938811	12.884493	-0.052123	4.815523
249.125877	7999.932229	12.889498	-0.052108	4.815521
248.819665	7999.913363	12.894503	-0.052052	4.815517
249.072617	7999.958102	12.899507	-0.052099	4.815529
249.078911	7999.883465	12.904512	-0.052100	4.815507
249.051164	7999.953522	12.909517	-0.052096	4.815528
249.165939	7999.955419	12.914522	-0.052117	4.815528
249.077887	7999.942253	12.919527	-0.052101	4.815524
249.469017	8000.014885	12.924531	-0.052174	4.815543
249.012756	7999.916667	12.929536	-0.052089	4.815517
249.161875	7999.934077	12.934541	-0.052117	4.815521
249.146939	7999.929582	12.939546	-0.052115	4.815520
249.085697	7999.921127	12.944551	-0.052104	4.815518
249.067546	7999.892015	12.949555	-0.052100	4.815509
248.923586	7999.864051	12.954560	-0.052074	4.815502
249.108943	7999.932251	12.959565	-0.052109	4.815521
249.012137	7999.934962	12.964570	-0.052091	4.815522
249.043730	7999.885303	12.969575	-0.052097	4.815508
249.136552	7999.991508	12.974579	-0.052115	4.815538
248.921887	7999.939960	12.979584	-0.052075	4.815524
249.282291	7999.883924	12.984589	-0.052142	4.815506
249.141377	7999.951065	12.989594	-0.052116	4.815526
249.179542	7999.947438	12.994599	-0.052124	4.815525
249.207860	7999.957534	12.999603	-0.052129	4.815528
249.248149	7999.952874	13.004608	-0.052137	4.815526
249.386255	7999.928451	13.009613	-0.052163	4.815518
249.068666	7999.948915	13.014618	-0.052104	4.815526
249.121276	7999.919891	13.019623	-0.052114	4.815517
249.259800	7999.970238	13.024627	-0.052140	4.815531
248.965661	7999.907779	13.029632	-0.052085	4.815514
249.199557	7999.955411	13.034637	-0.052129	4.815527
249.097823	7999.989015	13.039642	-0.052111	4.815537
249.141885	7999.924607	13.044647	-0.052119	4.815518
249.139062	7999.939534	13.049651	-0.052119	4.815523
249.011176	7999.944942	13.054656	-0.052095	4.815525
249.054180	7999.958483	13.059661	-0.052103	4.815529
249.063486	7999.981085	13.064666	-0.052105	4.815535
249.339005	7999.880941	13.069671	-0.052157	4.815505
249.349483	7999.972984	13.074675	-0.052159	4.815532
249.191732	7999.940523	13.079680	-0.052130	4.815523
249.096098	7999.952866	13.084685	-0.052112	4.815527
249.173041	7999.977641	13.089690	-0.052127	4.815534
249.162857	7999.857877	13.094695	-0.052125	4.815499
249.178982	7999.908359	13.099699	-0.052129	4.815513
249.087184	7999.939989	13.104704	-0.052112	4.815523
249.234956	7999.945629	13.109709	-0.052139	4.815524
249.247709	7999.956539	13.114714	-0.052142	4.815527
249.083462	7999.946400	13.119719	-0.052112	4.815525
249.249950	7999.994000	13.124723	-0.052143	4.815538
249.102255	7999.910437	13.129728	-0.052116	4.815514
249.300575	7999.882726	13.134733	-0.052153	4.815505
249.058190	7999.951413	13.139738	-0.052108	4.815527
249.107368	7999.922333	13.144743	-0.052117	4.815518
249.271614	7999.966691	13.149747	-0.052148	4.815530
248.963089	7999.927494	13.154752	-0.052091	4.815520
249.164793	7999.966056	13.159757	-0.052129	4.815530
249.265568	8000.008310	13.164762	-0.052148	4.815542
249.312459	7999.928994	13.169767	-0.052157	4.815519
249.302429	7999.997206	13.174771	-0.052155	4.815539
248.986588	7999.922644	13.179776	-0.052097	4.815518
248.906690	7999.892523	13.184781	-0.052082	4.815510
249.313414	7999.963272	13.189786	-0.052158	4.815529
249.121072	7999.933450	13.194791	-0.052122	4.815521
249.080631	7999.970191	13.199795	-0.052115	4.815532
249.055298	7999.912125	13.204800	-0.052111	4.815515
249.281829	7999.938277	13.209805	-0.052153	4.815522
249.131803	7999.989248	13.214810	-0.052125	4.815537
249.208458	7999.961685	13.219815	-0.052140	4.815529
249.494290	7999.968514	13.224819	-0.052193	4.815529
249.352707	7999.927772	13.229824	-0.052167	4.815518
249.156436	7999.920314	13.234829	-0.052131	4.815517
249.222691	7999.974819	13.239834	-0.052144	4.815532
249.237064	7999.889633	13.244839	-0.052146	4.815508
249.234848	7999.963312	13.249843	-0.052146	4.815529
249.178932	7999.982712	13.254848	-0.052136	4.815535
249.072325	7999.933998	13.259853	-0.052116	4.815521
249.194817	7999.961654	13.264858	-0.052140	4.815529
249.177661	7999.925082	13.269863	-0.052137	4.815518
249.299532	7999.958067	13.274867	-0.052160	4.815527
249.199601	7999.947911	13.279872	-0.052141	4.815525
249.087309	7999.921533	13.284877	-0.052120	4.815518
249.139560	7999.957653	13.289882	-0.052130	4.815528
249.058899	7999.898683	13.294887	-0.052116	4.815511
249.117175	8000.017140	13.299891	-0.052127	4.815545
249.194489	7999.921233	13.304896	-0.052141	4.815517
249.288553	7999.942017	13.309901	-0.052159	4.815523
249.319218	7999.977784	13.314906	-0.052165	4.815533
249.180501	7999.896504	13.319911	-0.052139	4.815510
249.360596	7999.985979	13.324915	-0.052173	4.815535
249.260471	7999.971548	13.329920	-0.052155	4.815531
249.265885	7999.960977	13.334925	-0.052156	4.815528
249.327821	7999.962011	13.339930	-0.052168	4.815528
249.300153	7999.912450	13.344935	-0.052163	4.815514
249.479773	7999.958128	13.349939	-0.052197	4.815526
249.263184	7999.932181	13.354944	-0.052157	4.815520
249.367619	7999.939249	13.359949	-0.052176	4.815521
249.324595	7999.987697	13.364954	-0.052169	4.815536
248.974406	7999.906166	13.369959	-0.052104	4.815513
249.310245	7999.997118	13.374963	-0.052166	4.815538
249.126440	7999.916169	13.379968	-0.052132	4.815516
249.181224	7999.924561	13.384973	-0.052143	4.815518
249.268047	7999.955907	13.389978	-0.052159	4.815527
249.189647	7999.932218	13.394983	-0.052145	4.815520
249.299927	7999.990647	13.399987	-0.052166	4.815537
249.376754	7999.951339	13.404992	-0.052180	4.815525
249.292475	7999.938234	13.409997	-0.052165	4.815521
249.478636	7999.993632	13.415002	-0.052200	4.815537
249.475761	7999.941272	13.420007	-0.052199	4.815521
249.363391	7999.959750	13.425011	-0.052179	4.815527
249.288108	7999.980970	13.430016	-0.052165	4.815534
249.215703	7999.906113	13.435021	-0.052152	4.815512
249.287743	7999.969258	13.440026	-0.052165	4.815530
249.218111	7999.985230	13.445031	-0.052153	4.815535
249.141047	8000.013897	13.450035	-0.052139	4.815544
249.162168	7999.961929	13.455040	-0.052143	4.815529
249.212102	7999.978787	13.460045	-0.052152	4.815533
249.123388	7999.967747	13.465050	-0.052136	4.815531
248.988047	7999.902542	13.470055	-0.052111	4.815512
249.230730	7999.939638	13.475059	-0.052156	4.815522
249.290843	7999.929962	13.480064	-0.052168	4.815519
249.234500	7999.869252	13.485069	-0.052158	4.815501
249.354721	7999.947069	13.490074	-0.052180	4.815523
249.499199	7999.868280	13.495079	-0.052207	4.815500
249.468477	7999.942562	13.500083	-0.052202	4.815522
249.306696	7999.916443	13.505088	-0.052172	4.815515
249.226892	7999.934384	13.510093	-0.052157	4.815520
249.504084	7999.977385	13.515098	-0.052209	4.815532
249.374921	7999.913349	13.520103	-0.052185	4.815513
249.522903	7999.971327	13.525107	-0.052213	4.815530
249.215546	7999.927876	13.530112	-0.052156	4.815518
249.216989	7999.921513	13.535117	-0.052157	4.815517
249.411160	7999.941796	13.540122	-0.052193	4.815522
249.298568	7999.896187	13.545127	-0.052172	4.815509
249.397412	7999.981131	13.550131	-0.052191	4.815533
249.382805	7999.964893	13.555136	-0.052189	4.815528
249.366872	7999.930477	13.560141	-0.052186	4.815518
249.396643	7999.982251	13.565146	-0.052192	4.815533
249.422756	7999.963474	13.570151	-0.052197	4.815528
249.407640	7999.987813	13.575155	-0.052194	4.815535
249.525918	7999.961998	13.580160	-0.052216	4.815527
249.398821	7999.891588	13.585165	-0.052193	4.815507
249.244326	7999.924330	13.590170	-0.052164	4.815517
249.587268	7999.902187	13.595175	-0.052229	4.815509
249.506368	7999.933995	13.600179	-0.052214	4.815519
249.134230	7999.895894	13.605184	-0.052145	4.815509
249.299370	7999.901818	13.610189	-0.052176	4.815510
249.558516	7999.950932	13.615194	-0.052224	4.815523
249.296517	7999.942399	13.620199	-0.052176	4.815522
249.315801	7999.958756	13.625203	-0.052180	4.815527
249.380828	7999.937411	13.630208	-0.052192	4.815520
249.321574	7999.922580	13.635213	-0.052181	4.815516
249.433258	7999.939379	13.640218	-0.052202	4.815521
249.268314	7999.918548	13.645223	-0.052172	4.815515
249.325082	7999.936585	13.650227	-0.052182	4.815520
249.223044	7999.862313	13.655232	-0.052164	4.815499
249.318359	7999.855347	13.660237	-0.052182	4.815497
249.352085	7999.937091	13.665242	-0.052188	4.815520
249.342443	7999.901709	13.670247	-0.052187	4.815510
249.402276	7999.957178	13.675251	-0.052198	4.815526
249.238523	7999.955591	13.680256	-0.052168	4.815526
249.195922	7999.943168	13.685261	-0.052160	4.815523
249.258700	7999.913242	13.690266	-0.052172	4.815514
249.238311	7999.924679	13.695271	-0.052168	4.815517
249.553297	7999.985386	13.700275	-0.052227	4.815533
249.266033	7999.964692	13.705280	-0.052174	4.815529
249.188647	7999.935679	13.710285	-0.052160	4.815521
249.372851	7999.966480	13.715290	-0.052195	4.815529
249.336601	7999.921051	13.720295	-0.052188	4.815516
249.334909	7999.972311	13.725299	-0.052188	4.815531
249.324527	7999.939053	13.730304	-0.052186	4.815521
249.550728	7999.954520	13.735309	-0.052229	4.815524
249.578788	7999.985973	13.740314	-0.052234	4.815533
249.488490	7999.963158	13.745319	-0.052218	4.815527
249.539929	7999.946931	13.750323	-0.052227	4.815522
249.362557	7999.959006	13.755328	-0.052195	4.815527
249.413456	7999.909661	13.760333	-0.052204	4.815512
249.626316	7999.994333	13.765338	-0.052244	4.815536
249.323660	7999.955230	13.770343	-0.052188	4.815526
249.257796	7999.919998	13.775347	-0.052176	4.815516
249.359982	7999.978295	13.780352	-0.052195	4.815532
249.340289	7999.955566	13.785357	-0.052192	4.815526
249.289620	7999.972916	13.790362	-0.052183	4.815531
249.331133	7999.865743	13.795367	-0.052191	4.815499
249.673937	7999.957879	13.800371	-0.052255	4.815525
249.513188	7999.951000	13.805376	-0.052225	4.815523
249.396967	7999.924557	13.810381	-0.052204	4.815516
249.654040	7999.982183	13.815386	-0.052252	4.815532
249.552073	7999.924999	13.820391	-0.052233	4.815516
249.634847	7999.923169	13.825395	-0.052249	4.815515
249.328916	7999.884013	13.830400	-0.052192	4.815505
249.460109	7999.933172	13.835405	-0.052217	4.815518
249.330759	7999.974869	13.840410	-0.052193	4.815531
249.167964	7999.991454	13.845415	-0.052163	4.815537
249.180609	7999.988478	13.850419	-0.052165	4.815536
249.325428	7999.962029	13.855424	-0.052192	4.815528
249.317579	7999.901044	13.860429	-0.052191	4.815510
249.341114	7999.975145	13.865434	-0.052196	4.815531
249.353606	7999.918764	13.870439	-0.052198	4.815515
249.508118	7999.989665	13.875443	-0.052227	4.815535
249.254004	7999.928927	13.880448	-0.052180	4.815518
249.272037	7999.898270	13.885453	-0.052184	4.815509
249.357910	7999.961641	13.890458	-0.052200	4.815527
249.314868	7999.858427	13.895463	-0.052192	4.815497
249.555403	7999.962776	13.900467	-0.052237	4.815527
249.454731	7999.954743	13.905472	-0.052219	4.815525
249.330288	7999.949526	13.910477	-0.052196	4.815524
249.474688	7999.997834	13.915482	-0.052223	4.815537
249.511116	7999.929027	13.920487	-0.052230	4.815517
249.464994	7999.972085	13.925491	-0.052222	4.815530
249.263775	7999.918619	13.930496	-0.052185	4.815515
249.372191	7999.895848	13.935501	-0.052205	4.815508
249.502325	7999.963146	13.940506	-0.052230	4.815527
249.502688	7999.966378	13.945511	-0.052230	4.815528
249.358316	7999.996081	13.950515	-0.052203	4.815537
249.353342	8000.004565	13.955520	-0.052203	4.815540
249.357824	7999.945917	13.960525	-0.052204	4.815523
249.338244	8000.018246	13.965530	-0.052200	4.815544
249.472187	7999.940353	13.970535	-0.052225	4.815520
249.578470	7999.965608	13.975539	-0.052245	4.815527
249.463540	7999.981908	13.980544	-0.052224	4.815532
249.549716	7999.958772	13.985549	-0.052241	4.815525
249.700452	8000.008252	13.990554	-0.052269	4.815539
249.499693	7999.957997	13.995559	-0.052232	4.815525
249.491441	7999.974973	14.000563	-0.052230	4.815530
249.610591	7999.976942	14.005568	-0.052253	4.815530
249.474935	7999.949112	14.010573	-0.052228	4.815523
249.623669	7999.956905	14.015578	-0.052256	4.815524
249.467621	7999.939423	14.020583	-0.052227	4.815520
249.510112	8000.017038	14.025587	-0.052235	4.815542
249.527277	7999.965006	14.030592	-0.052239	4.815527
249.474336	7999.920372	14.035597	-0.052229	4.815514
249.602636	7999.950259	14.040602	-0.052253	4.815523
249.452367	7999.988410	14.045607	-0.052225	4.815534
249.431966	8000.003051	14.050611	-0.052222	4.815539
249.357226	7999.959129	14.055616	-0.052208	4.815526
249.513721	7999.987341	14.060621	-0.052238	4.815534
249.669640	8000.015544	14.065626	-0.052267	4.815541
249.659082	7999.957718	14.070631	-0.052265	4.815524
249.440132	7999.985134	14.075635	-0.052225	4.815533
249.394167	7999.960907	14.080640	-0.052216	4.815527
249.542159	7999.888584	14.085645	-0.052244	4.815505
249.765951	8000.001204	14.090650	-0.052286	4.815537
249.308119	7999.962769	14.095655	-0.052201	4.815528
249.678807	7999.984870	14.100659	-0.052270	4.815532
249.612790	7999.956042	14.105664	-0.052258	4.815524
249.456581	7999.902244	14.110669	-0.052229	4.815509
249.534404	7999.907810	14.115674	-0.052244	4.815510
249.661881	7999.940888	14.120679	-0.052268	4.815519
249.617080	7999.935905	14.125683	-0.052260	4.815518
249.302575	7999.980984	14.130688	-0.052202	4.815533
249.488710	7999.976571	14.135693	-0.052236	4.815531
249.478575	7999.999924	14.140698	-0.052235	4.815537
249.369086	7999.981067	14.145703	-0.052215	4.815532
249.487431	7999.965934	14.150707	-0.052237	4.815528
249.588030	7999.983620	14.155712	-0.052256	4.815532
249.607194	7999.959389	14.160717	-0.052260	4.815525
249.475607	8000.011730	14.165722	-0.052236	4.815541
249.444129	7999.942882	14.170727	-0.052230	4.815521
249.655757	7999.997629	14.175731	-0.052270	4.815536
249.448450	8000.007078	14.180736	-0.052231	4.815540
249.477804	7999.945633	14.185741	-0.052237	4.815522
249.396264	7999.973158	14.190746	-0.052222	4.815530
249.205984	7999.967934	14.195751	-0.052187	4.815529
249.460748	8000.004160	14.200755	-0.052234	4.815539
249.597517	8000.002145	14.205760	-0.052260	4.815537
249.570945	7999.916288	14.210765	-0.052255	4.815513
249.488166	7999.975835	14.215770	-0.052240	4.815530
249.461504	7999.938039	14.220775	-0.052236	4.815519
249.702166	7999.953742	14.225779	-0.052281	4.815523
249.675830	7999.980035	14.230784	-0.052276	4.815531
249.755621	7999.969612	14.235789	-0.052291	4.815527
249.778326	8000.019135	14.240794	-0.052296	4.815542
249.848412	7999.922041	14.245799	-0.052309	4.815513
249.665235	7999.728956	14.250803	-0.052275	4.815457

249.631133	7996.405023	14.255808	-0.052266	4.814486
249.634010	7990.794646	14.260813	-0.052264	4.812845
249.394759	7984.054444	14.265818	-0.052215	4.810874
249.293652	7976.700669	14.270823	-0.052192	4.808723
249.414477	7969.060527	14.275827	-0.052209	4.806485
249.265733	7961.192795	14.280832	-0.052177	4.804181
249.214828	7953.350625	14.285837	-0.052162	4.801883
249.552599	7945.374369	14.290842	-0.052220	4.799543
249.286159	7937.472720	14.295847	-0.052166	4.797226
249.283068	7929.390621	14.300851	-0.052160	4.794854
249.342597	7921.403784	14.305856	-0.052166	4.792508
249.276130	7913.329806	14.310861	-0.052149	4.790137
249.118367	7905.441219	14.315866	-0.052115	4.787818
249.051643	7897.358248	14.320871	-0.052097	4.785442
249.275926	7889.471071	14.325875	-0.052134	4.783120
249.099566	7881.431682	14.330880	-0.052096	4.780754
248.970628	7873.399097	14.335885	-0.052067	4.778389
249.016649	7865.432156	14.340890	-0.052071	4.776041
248.934888	7857.356308	14.345895	-0.052051	4.773661
249.069302	7849.374046	14.350899	-0.052071	4.771306
248.646839	7841.341121	14.355904	-0.051987	4.768937
248.674363	7833.426784	14.360909	-0.051987	4.766600
248.852935	7825.366002	14.365914	-0.052015	4.764218
248.665893	7817.429451	14.370919	-0.051976	4.761873
248.789318	7809.368584	14.375923	-0.051994	4.759489
248.606164	7801.398913	14.380928	-0.051955	4.757132
248.518983	7793.344726	14.385933	-0.051933	4.754749
248.552877	7785.324426	14.390938	-0.051935	4.752373
248.520877	7777.290554	14.395943	-0.051924	4.749993
248.523471	7769.343230	14.400947	-0.051919	4.747637
248.617651	7761.329262	14.405952	-0.051932	4.745260
248.490114	7753.338019	14.410957	-0.051903	4.742889
248.434114	7745.387303	14.415962	-0.051888	4.740529
248.392364	7737.361907	14.420967	-0.051875	4.738146
248.409539	7729.305442	14.425971	-0.051873	4.735751
248.213106	7721.334981	14.430976	-0.051832	4.733382
248.117750	7713.296101	14.435981	-0.051809	4.730991
248.276986	7705.325546	14.440986	-0.051834	4.728618
248.277931	7697.310345	14.445991	-0.051829	4.726231
248.291328	7689.307692	14.450995	-0.051826	4.723847
247.958194	7681.366822	14.456000	-0.051759	4.721481
248.169506	7673.300702	14.461005	-0.051794	4.719075
248.319123	7665.376191	14.466010	-0.051817	4.716710
248.204894	7657.310246	14.471015	-0.051790	4.714302
248.066546	7649.308892	14.476019	-0.051760	4.711913
247.851295	7641.280781	14.481024	-0.051715	4.709514
247.928010	7633.309139	14.486029	-0.051724	4.707130
247.951743	7625.295219	14.491034	-0.051723	4.704733
247.858654	7617.289770	14.496039	-0.051701	4.702337
247.803833	7609.293920	14.501043	-0.051686	4.699943
247.828462	7601.323540	14.506048	-0.051685	4.697555
247.723848	7593.302228	14.511053	-0.051661	4.695151
247.657061	7585.319654	14.516058	-0.051644	4.692757
247.612866	7577.244590	14.521063	-0.051630	4.690334
247.843096	7569.282431	14.526067	-0.051668	4.687943
247.784562	7561.269605	14.531072	-0.051652	4.685536
247.670074	7553.292812	14.536077	-0.051626	4.683139
247.603416	7545.325601	14.541082	-0.051609	4.680743
247.681504	7537.276098	14.546087	-0.051618	4.678322
247.495103	7529.306165	14.551091	-0.051579	4.675923
247.482187	7521.254169	14.556096	-0.051571	4.673498
247.465807	7513.091366	14.561101	-0.051563	4.671039
247.474674	7505.192856	14.566106	-0.051560	4.668658
247.489755	7497.203204	14.571111	-0.051558	4.666248
247.596879	7489.226323	14.576115	-0.051573	4.663840
247.350851	7481.263559	14.581120	-0.051522	4.661436
247.219161	7473.216562	14.586125	-0.051492	4.659006
247.115136	7465.304032	14.591130	-0.051468	4.656614
247.220720	7457.198121	14.596135	-0.051483	4.654163
246.986335	7449.239844	14.601139	-0.051434	4.651755
246.985496	7441.202929	14.606144	-0.051429	4.649322
246.975330	7433.225852	14.611149	-0.051422	4.646906
247.057170	7425.204752	14.616154	-0.051432	4.644475
246.994968	7417.236917	14.621159	-0.051416	4.642059
247.030447	7409.182920	14.626163	-0.051418	4.639616
246.833959	7401.235564	14.631168	-0.051376	4.637204
246.867445	7393.174611	14.636173	-0.051377	4.634756
246.974530	7385.201228	14.641178	-0.051392	4.632333
246.841311	7377.134140	14.646183	-0.051362	4.629881
247.050235	7369.233888	14.651187	-0.051396	4.627478
246.694076	7361.164862	14.656192	-0.051325	4.625023
246.651792	7353.194790	14.661197	-0.051312	4.622596
246.598356	7345.200236	14.666202	-0.051297	4.620160
246.580205	7337.191504	14.671207	-0.051289	4.617719
246.595089	7329.198284	14.676211	-0.051287	4.615282
246.501419	7321.186794	14.681216	-0.051264	4.612837
246.446425	7313.135623	14.686221	-0.051249	4.610379
246.449757	7305.164362	14.691226	-0.051245	4.607944
246.453831	7297.153406	14.696231	-0.051241	4.605496
246.303401	7289.213196	14.701235	-0.051208	4.603068
246.222171	7281.180250	14.706240	-0.051187	4.600610
246.431350	7273.169628	14.711245	-0.051221	4.598158
246.456063	7265.189968	14.716250	-0.051221	4.595714
246.411845	7257.151514	14.721255	-0.051208	4.593251
246.364174	7249.088899	14.726259	-0.051194	4.590779
246.248458	7241.133554	14.731264	-0.051167	4.588339
245.927718	7233.094478	14.736269	-0.051103	4.585871
246.000491	7225.156482	14.741274	-0.051111	4.583433
245.897085	7217.119536	14.746279	-0.051087	4.580964
245.943667	7209.134268	14.751283	-0.051091	4.578509
245.837172	7201.141555	14.756288	-0.051066	4.576051
245.755150	7193.148038	14.761293	-0.051046	4.573590
245.807390	7185.095563	14.766298	-0.051051	4.571111
245.736886	7177.067132	14.771303	-0.051032	4.568637
245.920494	7169.139329	14.776307	-0.051062	4.566194
245.875381	7161.161966	14.781312	-0.051048	4.563733
245.859641	7153.175659	14.786317	-0.051040	4.561269
245.911453	7145.140823	14.791322	-0.051045	4.558788
245.696666	7137.167127	14.796327	-0.051000	4.556324
245.691856	7129.096873	14.801331	-0.050994	4.553830
245.702044	7121.105659	14.806336	-0.050991	4.551359
245.827055	7113.092986	14.811341	-0.051009	4.548879
245.733679	7105.154352	14.816346	-0.050987	4.546421
245.610647	7097.081174	14.821351	-0.050959	4.543920
245.265062	7089.134607	14.826355	-0.050890	4.541457
245.400606	7081.114174	14.831360	-0.050910	4.538970
245.431675	7073.129911	14.836365	-0.050911	4.536493
245.434633	7065.153197	14.841370	-0.050907	4.534016
245.440157	7057.087385	14.846375	-0.050903	4.531511
245.462246	7049.101247	14.851379	-0.050902	4.529029
245.353536	7041.120384	14.856384	-0.050877	4.526547
245.035371	7033.079220	14.861389	-0.050812	4.524044
245.244914	7025.174159	14.866394	-0.050846	4.521584
245.156875	7017.073132	14.871399	-0.050825	4.519060
245.095360	7009.133700	14.876403	-0.050809	4.516586
245.125696	7001.096839	14.881408	-0.050809	4.514080
245.134742	6993.012589	14.886413	-0.050806	4.511557
244.956638	6985.067377	14.891418	-0.050768	4.509077
244.777529	6977.042685	14.896423	-0.050729	4.506570
244.884889	6969.058022	14.901427	-0.050745	4.504075
244.939113	6961.105166	14.906432	-0.050750	4.501588
244.599797	6953.066458	14.911437	-0.050682	4.499072
244.675408	6945.103352	14.916442	-0.050691	4.496579
244.519902	6937.079048	14.921447	-0.050657	4.494065
244.466836	6929.053342	14.926451	-0.050642	4.491550
244.626037	6921.018143	14.931456	-0.050666	4.489031
244.632374	6913.041647	14.936461	-0.050663	4.486528
244.497029	6905.073033	14.941466	-0.050633	4.484026
244.643327	6897.071235	14.946471	-0.050655	4.481513
244.739740	6889.040635	14.951475	-0.050668	4.478990
244.370104	6881.116805	14.956480	-0.050594	4.476497
244.378426	6873.014852	14.961485	-0.050591	4.473948
244.502206	6865.047104	14.966490	-0.050609	4.471440
244.352331	6856.985815	14.971495	-0.050576	4.468900
244.353115	6849.031422	14.976499	-0.050571	4.466393
244.206804	6841.044625	14.981504	-0.050539	4.463874
244.378054	6833.039828	14.986509	-0.050566	4.461349
244.321038	6825.079832	14.991514	-0.050550	4.458836
244.144336	6817.011209	14.996519	-0.050512	4.456286
244.090603	6809.018820	15.001523	-0.050497	4.453760
243.930278	6801.001752	15.006528	-0.050462	4.451224
243.835128	6793.001307	15.011533	-0.050440	4.448692
243.928919	6785.023697	15.016538	-0.050452	4.446167
243.881296	6776.969704	15.021543	-0.050438	4.443615
243.819093	6769.039705	15.026547	-0.050422	4.441101
243.940253	6761.027092	15.031552	-0.050439	4.438561
243.854983	6753.063193	15.036557	-0.050419	4.436033
243.687703	6744.996897	15.041562	-0.050382	4.433471
243.676685	6736.934097	15.046567	-0.050375	4.430910
243.757212	6728.951236	15.051571	-0.050385	4.428372
243.748034	6720.976198	15.056576	-0.050379	4.425836
243.660806	6712.957864	15.061581	-0.050357	4.423283
243.710433	6705.023499	15.066586	-0.050362	4.420757
243.658974	6696.995276	15.071591	-0.050347	4.418199
243.622499	6688.990102	15.076595	-0.050335	4.415647
243.496787	6680.971399	15.081600	-0.050307	4.413088
243.470632	6672.899118	15.086605	-0.050297	4.410512
243.307999	6665.017483	15.091610	-0.050262	4.407994
243.201180	6656.967616	15.096615	-0.050237	4.405421
243.228053	6649.007192	15.101619	-0.050237	4.402876
243.237652	6640.997021	15.106624	-0.050234	4.400313
243.213280	6632.984289	15.111629	-0.050224	4.397748
243.307728	6625.021010	15.116634	-0.050237	4.395198
243.458092	6616.958134	15.121639	-0.050260	4.392615
243.209396	6608.919513	15.126643	-0.050209	4.390036
242.918635	6600.968170	15.131648	-0.050150	4.387483
243.156919	6592.935408	15.136653	-0.050189	4.384906
243.259679	6585.000066	15.141658	-0.050203	4.382357
242.891127	6576.953544	15.146663	-0.050130	4.379769
242.916003	6569.017310	15.151667	-0.050129	4.377216
242.971339	6561.008518	15.156672	-0.050135	4.374640
242.854881	6552.988253	15.161677	-0.050108	4.372056
242.845990	6544.968815	15.166682	-0.050101	4.369473
242.880100	6536.976547	15.171687	-0.050103	4.366896
242.844927	6528.958394	15.176691	-0.050091	4.364310
242.807360	6521.033060	15.181696	-0.050079	4.361752
242.687174	6512.940063	15.186701	-0.050052	4.359137
242.615204	6505.046122	15.191706	-0.050034	4.356586
242.451184	6496.961768	15.196711	-0.049998	4.353971
242.556968	6488.888462	15.201715	-0.050013	4.351360
242.500353	6480.888845	15.206720	-0.049997	4.348770
242.601087	6472.911014	15.211725	-0.050011	4.346186
242.806594	6464.991567	15.216730	-0.050044	4.343621
242.781924	6456.959332	15.221735	-0.050035	4.341016
242.498412	6448.995131	15.226739	-0.049977	4.338430
242.239872	6440.992009	15.231744	-0.049924	4.335829
242.229373	6432.952902	15.236749	-0.049917	4.333217
242.229339	6424.940508	15.241754	-0.049912	4.330613
242.073699	6416.946915	15.246759	-0.049878	4.328011
242.049784	6408.961032	15.251763	-0.049869	4.325412
241.960665	6400.981424	15.256768	-0.049847	4.322813
241.856044	6392.939965	15.261773	-0.049823	4.320191
241.767641	6384.972941	15.266778	-0.049801	4.317593
241.966424	6376.908508	15.271783	-0.049833	4.314963
242.083034	6368.923477	15.276787	-0.049850	4.312357
241.995789	6360.917415	15.281792	-0.049829	4.309741
241.917711	6352.912221	15.286797	-0.049809	4.307124
242.021373	6344.928616	15.291802	-0.049824	4.304514
242.104276	6336.925520	15.296807	-0.049834	4.301896
241.870864	6328.913925	15.301811	-0.049786	4.299270
241.966920	6321.007909	15.306816	-0.049799	4.296681
241.796259	6312.912298	15.311821	-0.049762	4.294025
241.823411	6304.932003	15.316826	-0.049762	4.291407
241.728441	6296.902565	15.321831	-0.049739	4.288771
241.763698	6288.919505	15.326835	-0.049741	4.286149
241.405681	6280.909475	15.331840	-0.049669	4.283513
241.306140	6272.935907	15.336845	-0.049646	4.280890
241.672663	6264.948681	15.341850	-0.049709	4.278265
241.416271	6256.915965	15.346855	-0.049656	4.275618
241.212388	6248.910649	15.351859	-0.049613	4.272978
241.397685	6240.867028	15.356864	-0.049643	4.270328
241.421878	6232.871379	15.361869	-0.049642	4.267691
241.374231	6224.892037	15.366874	-0.049628	4.265056
241.303837	6216.906923	15.371879	-0.049610	4.262418
241.515950	6208.888941	15.376883	-0.049645	4.259770
241.313590	6200.912620	15.381888	-0.049602	4.257130
241.228591	6192.893792	15.386893	-0.049581	4.254476
241.267798	6184.912401	15.391898	-0.049584	4.251834
241.236640	6176.855026	15.396903	-0.049573	4.249164
241.245563	6168.903281	15.401907	-0.049570	4.246527
241.154676	6160.912250	15.406912	-0.049548	4.243876
241.114697	6152.912591	15.411917	-0.049535	4.241220
241.042646	6144.989353	15.416922	-0.049517	4.238587
241.062983	6136.950101	15.421927	-0.049516	4.235915
240.887201	6128.955379	15.426931	-0.049478	4.233255
240.831654	6120.905051	15.431936	-0.049463	4.230575
240.722789	6112.908279	15.436941	-0.049438	4.227911
240.756853	6104.891773	15.441946	-0.049439	4.225240
240.669503	6096.945717	15.446951	-0.049418	4.222590
240.629130	6088.931256	15.451955	-0.049405	4.219916
240.611198	6081.010036	15.456960	-0.049397	4.217271
240.515112	6072.947618	15.461965	-0.049374	4.214577
240.457714	6064.902293	15.466970	-0.049358	4.211887
240.345098	6056.891825	15.471975	-0.049332	4.209206
240.345431	6048.924055	15.476979	-0.049328	4.206540
240.449481	6040.942280	15.481984	-0.049342	4.203868
240.287802	6032.937531	15.486989	-0.049307	4.201183
240.179169	6024.956779	15.491994	-0.049282	4.198506
240.059380	6016.967570	15.496999	-0.049254	4.195824
240.113650	6008.851572	15.502003	-0.049259	4.193099
240.010716	6000.814609	15.507008	-0.049235	4.190398
240.156799	5992.844473	15.512013	-0.049258	4.187720
240.189655	5984.888620	15.517018	-0.049259	4.185043
240.056956	5976.905239	15.522023	-0.049229	4.182354
240.306036	5968.879320	15.527027	-0.049270	4.179654
240.084866	5960.948086	15.532032	-0.049224	4.176978
239.840431	5952.882159	15.537037	-0.049174	4.174254
240.038805	5944.912232	15.542042	-0.049206	4.171567
240.023965	5936.908323	15.547047	-0.049198	4.168863
239.865306	5928.901547	15.552051	-0.049164	4.166156
240.050455	5920.907751	15.557056	-0.049193	4.163454
239.884289	5912.912630	15.562061	-0.049157	4.160747
239.718759	5904.915393	15.567066	-0.049121	4.158037
239.629054	5896.863717	15.572071	-0.049100	4.155308
239.821253	5888.876616	15.577075	-0.049130	4.152602
239.593284	5880.881733	15.582080	-0.049083	4.149887
239.490585	5872.874912	15.587085	-0.049059	4.147167
239.591588	5864.857928	15.592090	-0.049073	4.144445
239.461342	5856.937017	15.597095	-0.049044	4.141751
239.287288	5848.882514	15.602099	-0.049006	4.139009
239.491973	5840.913346	15.607104	-0.049039	4.136298
239.408139	5832.846126	15.612109	-0.049019	4.133549
239.584687	5824.861848	15.617114	-0.049047	4.130830
239.159508	5816.879097	15.622119	-0.048963	4.128102
239.227672	5808.872735	15.627123	-0.048970	4.125370
239.203868	5800.922565	15.632128	-0.048961	4.122655
239.030413	5792.869046	15.637133	-0.048924	4.119900
239.267997	5784.931614	15.642138	-0.048963	4.117189
239.251779	5776.887531	15.647143	-0.048955	4.114436
239.012602	5768.846303	15.652147	-0.048905	4.111679
239.222964	5760.834546	15.657152	-0.048940	4.108936
238.995520	5752.869286	15.662157	-0.048892	4.106202
239.048493	5744.869606	15.667162	-0.048897	4.103458
238.769191	5736.885303	15.672167	-0.048840	4.100713
238.884192	5728.895783	15.677171	-0.048857	4.097969
238.931968	5720.906013	15.682176	-0.048861	4.095223
238.746402	5712.869915	15.687181	-0.048821	4.092455
238.741779	5704.888446	15.692186	-0.048815	4.089707
238.741211	5696.901321	15.697191	-0.048810	4.086956
238.671795	5688.898770	15.702195	-0.048792	4.084196
238.772077	5680.952811	15.707200	-0.048806	4.081456
238.817413	5672.919425	15.712205	-0.048809	4.078683
238.690130	5664.967987	15.717210	-0.048781	4.075935
238.534944	5656.912052	15.722215	-0.048747	4.073148
238.472020	5648.888635	15.727219	-0.048730	4.070371
238.574884	5640.923474	15.732224	-0.048744	4.067615
238.448524	5632.902785	15.737229	-0.048716	4.064835
238.419606	5624.946658	15.742234	-0.048705	4.062077
238.281860	5616.930273	15.747239	-0.048675	4.059294
238.181731	5608.982622	15.752243	-0.048651	4.056534
238.204635	5600.943651	15.757248	-0.048651	4.053742
238.089370	5592.904333	15.762253	-0.048624	4.050946
238.189456	5584.962046	15.767258	-0.048638	4.048185
237.930691	5576.918378	15.772263	-0.048585	4.045382
238.026086	5568.954058	15.777267	-0.048597	4.042609
238.225117	5560.961198	15.782272	-0.048630	4.039826
237.967247	5552.976358	15.787277	-0.048577	4.037037
237.770586	5544.921193	15.792282	-0.048535	4.034223
237.659262	5536.781376	15.797287	-0.048509	4.031378
237.742588	5528.859443	15.802291	-0.048520	4.028610
237.835354	5520.860424	15.807296	-0.048532	4.025814
237.544231	5512.892678	15.812301	-0.048473	4.023020
237.629360	5504.912244	15.817306	-0.048484	4.020227
237.577723	5496.927349	15.822311	-0.048469	4.017427
237.436339	5488.910216	15.827315	-0.048438	4.014613
237.386142	5480.910706	15.832320	-0.048424	4.011804
237.119167	5472.899884	15.837325	-0.048369	4.008986
237.207337	5464.911682	15.842330	-0.048380	4.006180
237.280846	5456.897768	15.847335	-0.048389	4.003362
237.206672	5448.914795	15.852339	-0.048370	4.000551
237.211738	5440.949807	15.857344	-0.048366	3.997746
237.324171	5432.885449	15.862349	-0.048382	3.994905
237.534347	5424.904577	15.867354	-0.048416	3.992094
237.321844	5416.862112	15.872359	-0.048372	3.989251
237.075229	5408.910107	15.877363	-0.048321	3.986438
237.015512	5400.928638	15.882368	-0.048305	3.983616
236.907623	5392.892467	15.887373	-0.048280	3.980772
237.119800	5384.908783	15.892378	-0.048314	3.977949
237.094696	5376.933057	15.897383	-0.048305	3.975123
236.980437	5368.935544	15.902387	-0.048278	3.972286
236.878042	5360.916844	15.907392	-0.048254	3.969440
236.927059	5352.946830	15.912397	-0.048259	3.966612
237.096226	5344.945984	15.917402	-0.048285	3.963772
236.789617	5336.978957	15.922407	-0.048223	3.960934
236.797719	5328.977138	15.927411	-0.048220	3.958088
236.823233	5321.038090	15.932416	-0.048219	3.955262
236.735660	5312.946412	15.937421	-0.048198	3.952377
236.463557	5304.918721	15.942426	-0.048142	3.949510
236.756835	5296.914722	15.947431	-0.048192	3.946660
236.539420	5288.951160	15.952435	-0.048147	3.943812
236.455232	5280.999960	15.957440	-0.048126	3.940970
236.323447	5272.987079	15.962445	-0.048096	3.938102
236.506680	5265.001899	15.967450	-0.048126	3.935248
236.399267	5256.964647	15.972455	-0.048101	3.932368
236.250732	5248.939756	15.977459	-0.048068	3.929490
236.204695	5241.016592	15.982464	-0.048055	3.926647
236.265435	5232.945956	15.987469	-0.048061	3.923752
236.268750	5224.994532	15.992474	-0.048056	3.920896
236.075721	5217.032001	15.997479	-0.048016	3.918031
236.020917	5209.001497	16.002483	-0.048000	3.915142
235.944881	5200.989313	16.007488	-0.047981	3.912256
235.754408	5192.955192	16.012493	-0.047941	3.909359
235.928878	5185.003452	16.017498	-0.047968	3.906495
235.972385	5176.953546	16.022503	-0.047971	3.903592
235.816050	5168.964128	16.027507	-0.047937	3.900705
235.804779	5161.025797	16.032512	-0.047930	3.897837
235.903789	5152.971858	16.037517	-0.047944	3.894927
235.830846	5144.958848	16.042522	-0.047925	3.892026
235.844412	5136.945545	16.047527	-0.047923	3.889125
235.999666	5128.982370	16.052531	-0.047947	3.886242
235.905222	5121.004794	16.057536	-0.047924	3.883348
235.584247	5112.995458	16.062541	-0.047859	3.880435
235.732132	5105.049591	16.067546	-0.047882	3.877552
235.722467	5097.011594	16.072551	-0.047875	3.874630
235.357383	5088.760372	16.077555	-0.047802	3.871622
235.489307	5080.838538	16.082560	-0.047822	3.868741
235.450175	5072.873619	16.087565	-0.047810	3.865839
235.265189	5064.956066	16.092570	-0.047770	3.862949
235.240553	5056.944194	16.097575	-0.047761	3.860025
235.178414	5048.980647	16.102579	-0.047744	3.857117
235.441363	5040.974429	16.107584	-0.047788	3.854197
235.345473	5032.938594	16.112589	-0.047765	3.851256
235.186372	5024.983244	16.117594	-0.047731	3.848342
235.212903	5016.970796	16.122599	-0.047731	3.845408
235.319031	5008.986393	16.127603	-0.047745	3.842484
235.367790	5001.007852	16.132608	-0.047750	3.839559
235.067997	4993.032084	16.137613	-0.047689	3.836625
235.143863	4985.025993	16.142618	-0.047698	3.833686
235.021250	4977.020313	16.147623	-0.047670	3.830740
235.190281	4968.990653	16.152627	-0.047697	3.827789
234.956594	4961.042702	16.157632	-0.047648	3.824858
234.690177	4953.059634	16.162637	-0.047594	3.821911
234.981385	4945.071048	16.167642	-0.047643	3.818971
234.928965	4937.077903	16.172647	-0.047628	3.816020
234.666905	4929.054957	16.177651	-0.047574	3.813052
234.663494	4921.094259	16.182656	-0.047569	3.810109
234.682643	4913.072596	16.187661	-0.047567	3.807142
234.609346	4905.063439	16.192666	-0.047549	3.804176
234.579276	4897.122046	16.197671	-0.047538	3.801233
234.504245	4889.114561	16.202675	-0.047519	3.798263
234.511884	4881.125312	16.207680	-0.047516	3.795298
234.265735	4873.077526	16.212685	-0.047465	3.792304
234.397443	4865.022958	16.217690	-0.047484	3.789314
234.438626	4857.060651	16.222695	-0.047487	3.786353
234.324974	4849.069399	16.227699	-0.047461	3.783376
234.306187	4841.085494	16.232704	-0.047453	3.780401
234.306061	4833.106761	16.237709	-0.047448	3.777427
234.262910	4825.092593	16.242714	-0.047435	3.774435
233.992471	4817.076028	16.247719	-0.047379	3.771436
234.196428	4809.060471	16.252723	-0.047412	3.768445
234.023358	4801.076720	16.257728	-0.047375	3.765455
233.850810	4793.108530	16.262733	-0.047338	3.762468
233.805011	4785.102304	16.267738	-0.047324	3.759468
233.967291	4777.137948	16.272743	-0.047350	3.756486
234.047667	4769.093426	16.277747	-0.047360	3.753470
233.994697	4761.092699	16.282752	-0.047345	3.750464
233.976911	4753.077126	16.287757	-0.047337	3.747451
233.972554	4745.087088	16.292762	-0.047331	3.744446
233.794358	4737.145861	16.297767	-0.047293	3.741453
233.673391	4729.141206	16.302771	-0.047265	3.738434
233.730820	4721.155841	16.307776	-0.047271	3.735425
233.692618	4713.127521	16.312781	-0.047259	3.732395
233.672631	4705.112027	16.317786	-0.047250	3.729367
233.550767	4697.168984	16.322791	-0.047222	3.726362
233.545777	4689.097898	16.327795	-0.047216	3.723309
233.457080	4681.162448	16.332800	-0.047195	3.720303
233.241819	4673.189683	16.337805	-0.047150	3.717277
233.426775	4665.205988	16.342810	-0.047179	3.714255
233.244583	4657.073964	16.347815	-0.047141	3.711164
233.405394	4649.080245	16.352819	-0.047165	3.708132
233.357634	4641.132813	16.357824	-0.047152	3.705110
233.145191	4633.170624	16.362829	-0.047107	3.702076
233.272539	4625.164181	16.367834	-0.047126	3.699031
233.207645	4617.224374	16.372839	-0.047109	3.696003
233.200346	4609.191581	16.377843	-0.047103	3.692940
233.081662	4601.178527	16.382848	-0.047075	3.689878
232.942931	4593.219253	16.387853	-0.047045	3.686834
232.946055	4585.187836	16.392858	-0.047040	3.683764
232.985647	4577.216153	16.397863	-0.047043	3.680715
232.832745	4569.233747	16.402867	-0.047009	3.677654
232.832119	4561.240550	16.407872	-0.047004	3.674590
232.986690	4553.195621	16.412877	-0.047028	3.671508
233.022117	4545.186530	16.417882	-0.047030	3.668434
232.883091	4537.199155	16.422887	-0.046999	3.665362
232.954609	4529.230273	16.427891	-0.047007	3.662299
232.936020	4521.227116	16.432896	-0.046999	3.659218
232.877202	4513.243170	16.437901	-0.046983	3.656141
232.800298	4505.254260	16.442906	-0.046963	3.653059
232.555973	4497.231826	16.447911	-0.046913	3.649957
232.592565	4489.241497	16.452915	-0.046915	3.646872
232.459303	4481.261529	16.457920	-0.046885	3.643784
232.265182	4473.289363	16.462925	-0.046844	3.640695
232.265531	4465.317048	16.467930	-0.046839	3.637608
232.476201	4457.277323	16.472935	-0.046873	3.634498
232.398023	4449.233105	16.477939	-0.046854	3.631376
232.330011	4441.256234	16.482944	-0.046836	3.628278
232.322859	4433.226532	16.487949	-0.046830	3.625158
232.305821	4425.281487	16.492954	-0.046822	3.622069
232.030219	4417.302888	16.497959	-0.046765	3.618956
232.086734	4409.316668	16.502963	-0.046771	3.615847
232.164968	4401.307746	16.507968	-0.046781	3.612727
231.981478	4393.292283	16.512973	-0.046741	3.609594
232.024444	4385.344473	16.517978	-0.046744	3.606491
232.056997	4377.333174	16.522983	-0.046746	3.603361
231.869189	4369.346179	16.527987	-0.046706	3.600231
232.023345	4361.367206	16.532992	-0.046729	3.597111
231.972082	4353.358099	16.537997	-0.046715	3.593971
231.844822	4345.362293	16.543002	-0.046686	3.590831
231.738275	4337.369662	16.548007	-0.046661	3.587691
231.906693	4329.350654	16.553011	-0.046688	3.584545
231.683269	4321.404383	16.558016	-0.046641	3.581413
231.619666	4313.402783	16.563021	-0.046624	3.578262
231.403814	4305.441567	16.568026	-0.046579	3.575119
231.299337	4297.411234	16.573031	-0.046555	3.571950
231.487401	4289.340506	16.578035	-0.046585	3.568770
231.336356	4281.411669	16.583040	-0.046552	3.565634
230.961024	4273.423562	16.588045	-0.046477	3.562465
231.158801	4265.399530	16.593050	-0.046509	3.559295
231.201617	4257.479941	16.598055	-0.046512	3.556160
231.292931	4249.356682	16.603059	-0.046524	3.552942
231.020064	4241.330043	16.608064	-0.046468	3.549749
230.876115	4233.364761	16.613069	-0.046436	3.546582
231.023055	4225.396628	16.618074	-0.046459	3.543419
230.880379	4217.411828	16.623079	-0.046427	3.540238
230.782570	4209.444998	16.628083	-0.046404	3.537062
230.819225	4201.436847	16.633088	-0.046406	3.533872
230.623761	4193.406567	16.638093	-0.046364	3.530662
230.904510	4185.419415	16.643098	-0.046412	3.527482
230.813134	4177.403651	16.648103	-0.046390	3.524275
230.838743	4169.490053	16.653107	-0.046390	3.521110
230.641881	4161.492250	16.658112	-0.046348	3.517902
230.803413	4153.457211	16.663117	-0.046373	3.514687
230.554255	4145.475824	16.668122	-0.046322	3.511478
230.319331	4137.484432	16.673127	-0.046273	3.508262
230.469038	4129.444344	16.678131	-0.046296	3.505036
230.610701	4121.516956	16.683136	-0.046317	3.501852
230.411816	4113.506131	16.688141	-0.046275	3.498621
230.512828	4105.531331	16.693146	-0.046289	3.495410
230.601199	4097.523023	16.698151	-0.046301	3.492183
230.205983	4089.519738	16.703155	-0.046222	3.488940
230.271474	4081.551258	16.708160	-0.046229	3.485722
230.340054	4073.553605	16.713165	-0.046237	3.482489
230.410652	4065.585546	16.718170	-0.046245	3.479266
230.070349	4057.641919	16.723175	-0.046177	3.476036
230.093534	4049.582402	16.728179	-0.046176	3.472768
230.162210	4041.564517	16.733184	-0.046184	3.469515
230.072404	4033.556759	16.738189	-0.046162	3.466258
230.089117	4025.594871	16.743194	-0.046161	3.463021
230.026702	4017.613031	16.748199	-0.046144	3.459769
229.822960	4009.650062	16.753203	-0.046101	3.456517
229.805059	4001.659854	16.758208	-0.046093	3.453258
229.807718	3993.589179	16.763213	-0.046088	3.449963
229.892665	3985.623417	16.768218	-0.046099	3.446710
229.805299	3977.629506	16.773223	-0.046078	3.443438
229.708102	3969.652421	16.778227	-0.046055	3.440168
229.842740	3961.666392	16.783232	-0.046075	3.436900
229.864922	3953.661319	16.788237	-0.046074	3.433617
229.742027	3945.646119	16.793242	-0.046046	3.430321
229.859832	3937.663753	16.798247	-0.046063	3.427045
229.232966	3929.706899	16.803251	-0.045942	3.423750
229.377707	3921.723272	16.808256	-0.045964	3.420467
229.264765	3913.723845	16.813261	-0.045938	3.417166
229.414336	3905.722593	16.818266	-0.045960	3.413870
229.424616	3897.697485	16.823271	-0.045957	3.410556
229.281773	3889.715545	16.828275	-0.045926	3.407251
229.293310	3881.735347	16.833280	-0.045923	3.403949
229.096800	3873.756907	16.838285	-0.045881	3.400638
229.238802	3865.792628	16.843290	-0.045903	3.397341
229.183004	3857.776668	16.848295	-0.045888	3.394012
228.944916	3849.693790	16.853299	-0.045838	3.390646
229.051568	3841.731832	16.858304	-0.045853	3.387339
228.905061	3833.711273	16.863309	-0.045821	3.383995
228.884158	3825.777952	16.868314	-0.045812	3.380689
228.944763	3817.798356	16.873319	-0.045818	3.377363
228.937901	3809.797949	16.878323	-0.045812	3.374023
229.007806	3801.788476	16.883328	-0.045820	3.370678
228.495953	3793.853027	16.888333	-0.045720	3.367340
228.666963	3785.819536	16.893338	-0.045747	3.363983
228.777614	3777.860216	16.898343	-0.045762	3.360650
228.622128	3769.875105	16.903347	-0.045729	3.357295
228.509469	3761.899564	16.908352	-0.045703	3.353941
228.529907	3753.831492	16.913357	-0.045701	3.350550
228.328176	3745.855327	16.918362	-0.045659	3.347186
228.334352	3737.857386	16.923367	-0.045655	3.343817
228.193654	3729.891380	16.928371	-0.045624	3.340453
228.398578	3721.913695	16.933376	-0.045657	3.337093
228.149051	3713.910537	16.938381	-0.045606	3.333702
228.207003	3705.902743	16.943386	-0.045612	3.330317
228.333561	3697.919894	16.948391	-0.045630	3.326942
228.166584	3689.931880	16.953395	-0.045594	3.323550
227.886592	3682.017223	16.958400	-0.045537	3.320182
228.008255	3674.003258	16.963405	-0.045555	3.316783
228.086323	3665.966815	16.968410	-0.045564	3.313369
227.738381	3657.967610	16.973415	-0.045494	3.309952
227.786291	3649.992186	16.978419	-0.045498	3.306556
227.974758	3641.986072	16.983424	-0.045529	3.303149
227.765907	3634.015565	16.988429	-0.045485	3.299739
227.742919	3626.049185	16.993434	-0.045475	3.296333
227.684578	3618.033678	16.998439	-0.045460	3.292902
227.422818	3610.037550	17.003443	-0.045406	3.289468
227.569922	3602.097519	17.008448	-0.045428	3.286070
227.532328	3594.060140	17.013453	-0.045416	3.282620
227.675458	3586.057745	17.018458	-0.045438	3.279188
227.508351	3578.129513	17.023463	-0.045402	3.275772
227.240869	3570.083927	17.028467	-0.045347	3.272298
227.297590	3562.098605	17.033472	-0.045353	3.268859
227.208243	3554.094480	17.038477	-0.045331	3.265403
227.307824	3546.124237	17.043482	-0.045345	3.261965
227.331141	3538.131804	17.048487	-0.045344	3.258511
227.397374	3530.130921	17.053491	-0.045352	3.255051
227.204371	3522.176046	17.058496	-0.045311	3.251597
226.861803	3514.153571	17.063501	-0.045242	3.248104
226.987604	3506.139753	17.068506	-0.045260	3.244630
226.814371	3498.232499	17.073511	-0.045223	3.241186
226.764456	3490.234801	17.078515	-0.045209	3.237705
226.998547	3482.210020	17.083520	-0.045248	3.234219
226.980299	3474.139281	17.088525	-0.045239	3.230699
226.742365	3466.177203	17.093530	-0.045190	3.227214
226.611630	3458.223815	17.098535	-0.045161	3.223733
226.635736	3450.245311	17.103539	-0.045160	3.220244
226.737389	3442.289539	17.108544	-0.045174	3.216765
226.472739	3434.265769	17.113549	-0.045120	3.213236
226.686436	3426.244227	17.118554	-0.045155	3.209724
226.661873	3418.293647	17.123559	-0.045145	3.206230
226.558545	3410.324446	17.128563	-0.045121	3.202721
226.612768	3402.334203	17.133568	-0.045126	3.199205
226.438326	3394.353226	17.138573	-0.045089	3.195679
226.382586	3386.350744	17.143578	-0.045073	3.192146
226.113907	3378.362651	17.148583	-0.045018	3.188605
226.251696	3370.322107	17.153587	-0.045039	3.185055
226.269101	3362.402069	17.158592	-0.045037	3.181549
226.209198	3354.405967	17.163597	-0.045021	3.178002
226.050034	3346.416423	17.168602	-0.044987	3.174450
226.031208	3338.428691	17.173607	-0.044978	3.170900
225.944059	3330.410214	17.178611	-0.044957	3.167330
226.227634	3322.409080	17.183616	-0.045005	3.163780
225.854018	3314.484742	17.188621	-0.044930	3.160232
225.824196	3306.494822	17.193626	-0.044920	3.156665
225.863589	3298.482765	17.198631	-0.044922	3.153087
225.922789	3290.447856	17.203635	-0.044928	3.149496
225.882631	3282.491724	17.208640	-0.044916	3.145931
225.612563	3274.511476	17.213645	-0.044860	3.142342
225.691812	3266.519401	17.218650	-0.044870	3.138758
225.564434	3258.557433	17.223655	-0.044842	3.135175
225.473525	3250.550405	17.228659	-0.044820	3.131569
225.476671	3242.572458	17.233664	-0.044815	3.127977
225.479068	3234.553927	17.238669	-0.044811	3.124361
225.410333	3226.626381	17.243674	-0.044793	3.120780
225.379069	3218.651777	17.248679	-0.044782	3.117174
225.245030	3210.631822	17.253683	-0.044752	3.113540
225.342722	3202.625058	17.258688	-0.044765	3.109917
225.201279	3194.639771	17.263693	-0.044734	3.106290
225.160053	3186.674470	17.268698	-0.044722	3.102671
224.893134	3178.707485	17.273703	-0.044667	3.099038
224.966767	3170.688337	17.278707	-0.044676	3.095391
225.083997	3162.713246	17.283712	-0.044693	3.091763
225.034487	3154.689726	17.288717	-0.044678	3.088101
225.014433	3146.700784	17.293722	-0.044670	3.084451
225.152097	3138.763339	17.298727	-0.044690	3.080828
225.046914	3130.792327	17.303731	-0.044666	3.077174
225.107241	3122.772491	17.308736	-0.044672	3.073501
224.675735	3114.733429	17.313741	-0.044587	3.069792
224.546062	3106.776052	17.318746	-0.044558	3.066129
224.728863	3098.786811	17.323751	-0.044587	3.062463
224.561190	3090.810422	17.328755	-0.044550	3.058781
224.656229	3082.865485	17.333760	-0.044563	3.055122
224.560276	3074.855038	17.338765	-0.044540	3.051420
224.664814	3066.853289	17.343770	-0.044555	3.047726
224.483208	3058.890716	17.348775	-0.044516	3.044033
224.270826	3050.933675	17.353779	-0.044472	3.040335
224.365723	3042.969394	17.358784	-0.044484	3.036645
224.373877	3034.937767	17.363789	-0.044481	3.032915
224.452505	3026.936198	17.368794	-0.044491	3.029198
224.504836	3018.955192	17.373799	-0.044495	3.025484
224.218639	3010.987159	17.378803	-0.044437	3.021755
224.052801	3003.047942	17.383808	-0.044401	3.018042
224.352961	2995.009031	17.388813	-0.044452	3.014299
224.164966	2987.030500	17.393818	-0.044412	3.010557
223.735149	2979.100062	17.398823	-0.044327	3.006820
223.883840	2971.073556	17.403827	-0.044350	3.003062
224.127107	2963.084242	17.408832	-0.044390	2.999321
223.978463	2955.142875	17.413837	-0.044358	2.995579
223.886531	2947.106114	17.418842	-0.044336	2.991790
224.133912	2939.101823	17.423847	-0.044377	2.988029
224.049105	2931.110400	17.428851	-0.044356	2.984252
223.926687	2923.183310	17.433856	-0.044328	2.980499
223.860659	2915.200921	17.438861	-0.044311	2.976718
223.923161	2907.195882	17.443866	-0.044318	2.972928
223.854537	2899.191383	17.448871	-0.044300	2.969127
223.664418	2891.228589	17.453875	-0.044260	2.965334
223.575931	2883.285495	17.458880	-0.044238	2.961551
223.362492	2875.323468	17.463885	-0.044193	2.957748
223.315267	2867.320509	17.468890	-0.044180	2.953929
223.290717	2859.306530	17.473895	-0.044170	2.950101
223.368806	2851.301648	17.478899	-0.044180	2.946277
223.477893	2843.332429	17.483904	-0.044195	2.942468
223.258312	2835.351242	17.488909	-0.044149	2.938630
223.472800	2827.365876	17.493914	-0.044184	2.934808
223.406336	2819.388312	17.498919	-0.044167	2.930970
223.309317	2811.412899	17.503923	-0.044144	2.927127
223.476634	2803.416515	17.508928	-0.044170	2.923282
223.160192	2795.466750	17.513933	-0.044106	2.919429
223.296716	2787.503118	17.518938	-0.044127	2.915588
223.213656	2779.454109	17.523943	-0.044106	2.911690
223.263414	2771.437359	17.528947	-0.044110	2.907808
223.055705	2763.492490	17.533952	-0.044067	2.903943
222.857985	2755.537939	17.538957	-0.044025	2.900068
222.868622	2747.567849	17.543962	-0.044022	2.896192
222.791859	2739.568796	17.548967	-0.044003	2.892292
222.694114	2731.583545	17.553971	-0.043980	2.888392
222.754447	2723.599204	17.558976	-0.043986	2.884495
222.724723	2715.656072	17.563981	-0.043975	2.880609
222.770933	2707.672511	17.568986	-0.043979	2.876702
222.700376	2699.703928	17.573991	-0.043961	2.872790
222.680031	2691.663734	17.578995	-0.043952	2.868841
222.588059	2683.728312	17.584000	-0.043930	2.864934
222.390147	2675.761190	17.589005	-0.043888	2.861000
222.505983	2667.787508	17.594010	-0.043905	2.857074
222.441171	2659.802138	17.599015	-0.043888	2.853128
222.249847	2651.786627	17.604019	-0.043847	2.849154
222.515530	2643.815091	17.609024	-0.043892	2.845222
222.450892	2635.847218	17.614029	-0.043875	2.841267
222.448145	2627.861450	17.619034	-0.043869	2.837302
222.248751	2619.898557	17.624039	-0.043827	2.833332
221.960062	2611.908867	17.629043	-0.043769	2.829337
221.975954	2603.927124	17.634048	-0.043767	2.825358
221.754865	2595.972473	17.639053	-0.043721	2.821373
221.776704	2588.005716	17.644058	-0.043720	2.817391
222.090784	2579.986767	17.649063	-0.043773	2.813394
221.815068	2571.995825	17.654067	-0.043717	2.809371
221.681887	2564.052874	17.659072	-0.043687	2.805374
221.528289	2556.082104	17.664077	-0.043654	2.801357
221.578694	2548.104857	17.669082	-0.043658	2.797342
221.699020	2540.113622	17.674087	-0.043675	2.793319
221.518812	2532.103196	17.679091	-0.043637	2.789262
221.638721	2524.133819	17.684096	-0.043654	2.785238
221.475959	2516.191522	17.689101	-0.043619	2.781206
221.441996	2508.216923	17.694106	-0.043608	2.777158
221.435365	2500.232970	17.699111	-0.043602	2.773102
221.186509	2492.239958	17.704115	-0.043550	2.769021
221.169335	2484.289297	17.709120	-0.043542	2.764969
221.193822	2476.314233	17.714125	-0.043542	2.760901
221.040176	2468.372441	17.719130	-0.043508	2.756833
221.038165	2460.325865	17.724135	-0.043503	2.752715
221.075268	2452.279417	17.729139	-0.043505	2.748593
221.064019	2444.320005	17.734144	-0.043498	2.744506
220.881884	2436.381125	17.739149	-0.043459	2.740414
221.020380	2428.422899	17.744154	-0.043480	2.736325
221.078984	2420.438774	17.749159	-0.043486	2.732212
220.866695	2412.447472	17.754163	-0.043441	2.728072
220.930878	2404.493423	17.759168	-0.043448	2.723962
220.911504	2396.534799	17.764173	-0.043440	2.719839
220.703125	2388.601797	17.769178	-0.043396	2.715711
220.603418	2380.615740	17.774183	-0.043372	2.711555
220.508251	2372.612659	17.779187	-0.043350	2.707385
220.690229	2364.619241	17.784192	-0.043379	2.703230
220.504752	2356.662434	17.789197	-0.043339	2.699066
220.275432	2348.716724	17.794202	-0.043291	2.694897
220.115822	2340.757157	17.799207	-0.043257	2.690720
220.050386	2332.755244	17.804211	-0.043240	2.686519
220.375901	2324.762554	17.809216	-0.043295	2.682342
220.180698	2316.837485	17.814221	-0.043254	2.678161
220.025275	2308.856723	17.819226	-0.043220	2.673946
220.022782	2300.835761	17.824231	-0.043215	2.669713
219.947265	2292.854702	17.829235	-0.043196	2.665490
220.061245	2284.917446	17.834240	-0.043212	2.661296
219.984606	2276.927654	17.839245	-0.043193	2.657055
219.923992	2268.962797	17.844250	-0.043176	2.652821
219.902047	2260.982787	17.849255	-0.043167	2.648575
219.750337	2253.004273	17.854259	-0.043134	2.644314
219.792519	2245.071000	17.859264	-0.043137	2.640084
219.709544	2237.102491	17.864269	-0.043117	2.635819
219.960620	2229.075454	17.869274	-0.043158	2.631538
219.659509	2221.139376	17.874279	-0.043097	2.627263
219.676214	2213.149800	17.879283	-0.043096	2.622973
219.686107	2205.205146	17.884288	-0.043093	2.618699
219.258613	2197.284854	17.889293	-0.043008	2.614403
219.365343	2189.270732	17.894298	-0.043023	2.610084
219.260686	2181.299275	17.899303	-0.042998	2.605768
219.103384	2173.346492	17.904307	-0.042964	2.601450
219.251234	2165.372947	17.909312	-0.042987	2.597135
219.321435	2157.278745	17.914317	-0.042995	2.592742
219.303314	2149.209269	17.919322	-0.042986	2.588348
219.172808	2141.302900	17.924327	-0.042957	2.584029
218.952763	2133.386794	17.929331	-0.042911	2.579691
219.130800	2125.434072	17.934336	-0.042940	2.575353
218.779950	2117.502043	17.939341	-0.042869	2.570982
218.781311	2109.525076	17.944346	-0.042865	2.566603
218.993142	2101.550444	17.949351	-0.042899	2.562233
218.704622	2093.617191	17.954355	-0.042840	2.557844
218.822582	2085.643110	17.959360	-0.042857	2.553453
218.837265	2077.639900	17.964365	-0.042855	2.549031
218.324897	2069.724592	17.969370	-0.042755	2.544612
218.480785	2061.767522	17.974375	-0.042779	2.540210
218.446783	2053.789118	17.979379	-0.042768	2.535775
218.505113	2045.808134	17.984384	-0.042774	2.531338
218.294514	2037.858147	17.989389	-0.042729	2.526890
218.314673	2029.877369	17.994394	-0.042728	2.522434
218.355921	2021.933893	17.999399	-0.042731	2.517993
218.423505	2013.936463	18.004403	-0.042739	2.513516
218.148933	2005.977805	18.009408	-0.042683	2.509027
218.315893	1997.963638	18.014413	-0.042709	2.504531
218.392031	1990.022242	18.019418	-0.042718	2.500062
218.176903	1982.101134	18.024423	-0.042673	2.495574
218.141852	1974.108221	18.029427	-0.042661	2.491052
218.119642	1966.159004	18.034432	-0.042652	2.486546
217.879193	1958.219279	18.039437	-0.042603	2.482022
217.755733	1950.268270	18.044442	-0.042575	2.477492
218.041951	1942.260750	18.049447	-0.042623	2.472951
217.861406	1934.301821	18.054451	-0.042584	2.468395
217.734142	1926.359736	18.059456	-0.042556	2.463845
217.693172	1918.403689	18.064461	-0.042543	2.459284
217.694626	1910.445177	18.069466	-0.042539	2.454717
217.686144	1902.458562	18.074471	-0.042532	2.450124
217.388664	1894.517833	18.079475	-0.042472	2.445527
217.600942	1886.557596	18.084480	-0.042506	2.440949
217.587693	1878.593039	18.089485	-0.042499	2.436343
217.417268	1870.572215	18.094490	-0.042462	2.431683
217.650339	1862.569447	18.099495	-0.042501	2.427056
217.329001	1854.648960	18.104499	-0.042436	2.422425
217.183761	1846.737880	18.109504	-0.042404	2.417804
217.250900	1838.747849	18.114509	-0.042411	2.413145
217.150050	1830.781653	18.119514	-0.042388	2.408477
217.082859	1822.839515	18.124519	-0.042370	2.403818
216.721281	1814.933713	18.129523	-0.042298	2.399147
216.969676	1806.961337	18.134528	-0.042339	2.394476
216.755733	1798.978834	18.139533	-0.042295	2.389754
216.793302	1791.008678	18.144538	-0.042297	2.385049
216.881674	1783.059788	18.149543	-0.042308	2.380352
216.768733	1775.097528	18.154547	-0.042282	2.375621
216.872510	1767.118651	18.159552	-0.042296	2.370888
216.631391	1759.183192	18.164557	-0.042247	2.366145
216.674567	1751.228087	18.169562	-0.042250	2.361402
216.505077	1743.321804	18.174567	-0.042213	2.356662
216.505713	1735.304915	18.179571	-0.042208	2.351860
216.587136	1727.335541	18.184576	-0.042219	2.347084
216.529902	1719.393083	18.189581	-0.042203	2.342302
216.492951	1711.448851	18.194586	-0.042191	2.337512
216.632195	1703.471660	18.199591	-0.042212	2.332706
216.196872	1695.564802	18.204595	-0.042126	2.327885
215.935603	1687.638015	18.209600	-0.042073	2.323056
215.876529	1679.689489	18.214605	-0.042057	2.318221
216.074720	1671.689625	18.219610	-0.042089	2.313366
215.805503	1663.750469	18.224615	-0.042034	2.308499
215.840623	1655.769162	18.229619	-0.042035	2.303621
216.036680	1647.825122	18.234624	-0.042067	2.298770
215.976580	1639.878080	18.239629	-0.042051	2.293884
215.825346	1631.905561	18.244634	-0.042018	2.288965
215.968930	1623.945780	18.249639	-0.042039	2.284068
216.016621	1616.010394	18.254643	-0.042043	2.279167
215.770904	1608.101378	18.259648	-0.041993	2.274247
215.567631	1600.079167	18.264653	-0.041950	2.269250
215.609877	1592.112646	18.269658	-0.041953	2.264297
215.797425	1584.167099	18.274663	-0.041983	2.259359
215.496660	1576.259500	18.279667	-0.041922	2.254392
215.460096	1568.309338	18.284672	-0.041910	2.249410
215.448750	1560.325338	18.289677	-0.041903	2.244398
215.518453	1552.410811	18.294682	-0.041911	2.239426
215.250471	1544.515742	18.299687	-0.041856	2.234425
215.287771	1536.510160	18.304691	-0.041858	2.229370
214.925372	1528.607034	18.309696	-0.041786	2.224332
214.879235	1520.667585	18.314701	-0.041772	2.219289
215.268206	1512.666664	18.319706	-0.041840	2.214233
215.109984	1504.729686	18.324711	-0.041805	2.209158
214.729135	1496.813144	18.329715	-0.041729	2.204065
214.979031	1488.868733	18.334720	-0.041771	2.198998
215.104469	1480.891305	18.339725	-0.041789	2.193887
215.140045	1472.906799	18.344730	-0.041791	2.188752
215.058182	1464.987601	18.349735	-0.041771	2.183636
214.812711	1457.075496	18.354739	-0.041720	2.178497
214.915269	1449.138059	18.359744	-0.041735	2.173362
214.676617	1441.201361	18.364749	-0.041685	2.168184
214.408539	1433.273607	18.369754	-0.041630	2.162996
214.553118	1425.328864	18.374759	-0.041652	2.157823
214.366711	1417.390769	18.379763	-0.041613	2.152612
214.401352	1409.433977	18.384768	-0.041614	2.147395
214.130863	1401.513863	18.389773	-0.041559	2.142162
214.158918	1393.567623	18.394778	-0.041559	2.136927
214.052102	1385.636830	18.399783	-0.041534	2.131676
214.101469	1377.664105	18.404787	-0.041539	2.126399
214.265656	1369.731202	18.409792	-0.041564	2.121147
214.128178	1361.817982	18.414797	-0.041534	2.115866
214.110239	1353.808996	18.419802	-0.041525	2.110519
214.068469	1345.864285	18.424807	-0.041513	2.105199
213.781734	1337.967694	18.429811	-0.041454	2.099875
213.861234	1330.053534	18.434816	-0.041464	2.094560
213.938468	1322.076002	18.439821	-0.041474	2.089189
213.676765	1314.175779	18.444826	-0.041420	2.083823
213.542052	1306.281048	18.449831	-0.041390	2.078460
213.702571	1298.318320	18.454835	-0.041415	2.073066
213.703300	1290.364477	18.459840	-0.041410	2.067647
213.519940	1282.454020	18.464845	-0.041371	2.062226
213.417375	1274.543554	18.469850	-0.041347	2.056799
213.262490	1266.618779	18.474855	-0.041313	2.051342
213.215812	1258.669424	18.479859	-0.041300	2.045864
213.306229	1250.742686	18.484864	-0.041312	2.040401
213.183818	1242.843608	18.489869	-0.041284	2.034922
213.101585	1234.880227	18.494874	-0.041264	2.029386
213.110763	1226.945290	18.499879	-0.041261	2.023865
213.284679	1218.994695	18.504883	-0.041288	2.018335
213.180293	1211.088159	18.509888	-0.041264	2.012791
212.865410	1203.179750	18.514893	-0.041200	2.007209
212.780503	1195.269222	18.519898	-0.041179	2.001634
212.888094	1187.353309	18.524903	-0.041194	1.996060
212.754219	1179.406501	18.529907	-0.041165	1.990423
212.726832	1171.491702	18.534912	-0.041155	1.984803
212.690992	1163.574504	18.539917	-0.041143	1.979165
212.615879	1155.665193	18.544922	-0.041124	1.973513
212.308231	1147.770622	18.549927	-0.041062	1.967830
212.491835	1139.806495	18.554931	-0.041091	1.962133
212.703001	1131.886956	18.559936	-0.041126	1.956455
212.591426	1123.945766	18.564941	-0.041100	1.950709
212.245108	1116.044118	18.569946	-0.041030	1.944950
212.564023	1108.095958	18.574951	-0.041085	1.939212
212.281283	1100.217934	18.579955	-0.041027	1.933443
212.229052	1092.290701	18.584960	-0.041013	1.927645
212.137690	1084.383235	18.589965	-0.040991	1.921841
212.020022	1076.498800	18.594970	-0.040964	1.916032
211.950549	1068.580100	18.599975	-0.040946	1.910186
211.810326	1060.657814	18.604979	-0.040915	1.904312
211.959339	1052.741193	18.609984	-0.040938	1.898456
211.769521	1044.849395	18.614989	-0.040898	1.892562
211.541992	1036.938348	18.619994	-0.040850	1.886631
211.687556	1029.019265	18.624999	-0.040873	1.880718
211.685533	1021.118375	18.630003	-0.040867	1.874783
211.463890	1013.217252	18.635008	-0.040821	1.868803
211.664939	1005.257806	18.640013	-0.040854	1.862809
211.459864	997.394944	18.645018	-0.040811	1.856822
211.103667	989.531166	18.650023	-0.040739	1.850797
211.104414	981.595034	18.655027	-0.040735	1.844739
211.079107	973.722301	18.660032	-0.040725	1.838707
211.081773	965.810446	18.665037	-0.040721	1.832628
210.895869	957.907947	18.670042	-0.040681	1.826513
211.007174	949.993876	18.675047	-0.040697	1.820404
210.903162	942.115365	18.680051	-0.040673	1.814277
210.693493	934.232626	18.685056	-0.040629	1.808113
210.793290	926.309292	18.690061	-0.040642	1.801933
210.735097	918.431118	18.695066	-0.040627	1.795748
210.923836	910.455647	18.700071	-0.040657	1.789496
210.485475	902.612320	18.705075	-0.040570	1.783249
210.480085	894.730498	18.710080	-0.040564	1.777003
210.237023	886.867297	18.715085	-0.040514	1.770720
210.454292	878.929387	18.720090	-0.040550	1.764412
210.542619	871.057048	18.725095	-0.040561	1.758118
210.456780	863.169609	18.730099	-0.040540	1.751768
210.159197	855.318432	18.735104	-0.040480	1.745397
210.100851	847.442902	18.740109	-0.040464	1.739013
210.137681	839.541680	18.745114	-0.040466	1.732597
210.108817	831.659705	18.750119	-0.040456	1.726164
209.902440	823.805874	18.755123	-0.040413	1.719707
210.062573	815.915847	18.760128	-0.040438	1.713244
209.835792	808.038350	18.765133	-0.040391	1.706716
209.631054	800.180155	18.770138	-0.040348	1.700182
209.691839	792.302498	18.775143	-0.040354	1.693642
209.649460	784.396982	18.780147	-0.040341	1.687039
209.723179	776.529118	18.785152	-0.040350	1.680457
209.660412	768.681724	18.790157	-0.040333	1.673848
209.430769	760.828347	18.795162	-0.040286	1.667186
209.449558	752.950700	18.800167	-0.040284	1.660510
209.146568	745.128580	18.805171	-0.040223	1.653810
209.191606	737.243960	18.810176	-0.040227	1.647077
209.245929	729.367479	18.815181	-0.040232	1.640325
209.123884	721.517485	18.820186	-0.040204	1.633543
209.202474	713.590133	18.825191	-0.040214	1.626694
209.088453	705.749248	18.830195	-0.040188	1.619864
209.221058	697.887148	18.835200	-0.040208	1.613022
208.875403	690.069343	18.840205	-0.040139	1.606121
208.839612	682.231414	18.845210	-0.040127	1.599218
208.789786	674.395548	18.850215	-0.040113	1.592283
208.715890	666.527852	18.855219	-0.040094	1.585287
208.886925	658.674098	18.860224	-0.040121	1.578308
208.876502	650.819250	18.865229	-0.040114	1.571270
208.495453	643.035002	18.870234	-0.040039	1.564210
208.389118	635.220953	18.875239	-0.040014	1.557131
208.354279	627.350970	18.880243	-0.040003	1.549980
208.325425	619.511170	18.885248	-0.039992	1.542824
208.239022	611.687467	18.890253	-0.039971	1.535641
208.075312	603.862716	18.895258	-0.039936	1.528411
208.256275	596.009412	18.900263	-0.039965	1.521172
208.172574	588.199784	18.905267	-0.039944	1.513900
208.039338	580.384588	18.910272	-0.039915	1.506579
208.011111	572.563916	18.915277	-0.039905	1.499234
207.962901	564.752586	18.920282	-0.039891	1.491858
207.979100	556.922657	18.925287	-0.039889	1.484438
207.726835	549.155150	18.930291	-0.039837	1.476999
207.556958	541.329729	18.935296	-0.039801	1.469478
207.410609	533.510840	18.940301	-0.039769	1.461930
207.486883	525.691625	18.945306	-0.039778	1.454377
207.356980	517.900977	18.950311	-0.039749	1.446779
207.273412	510.109432	18.955315	-0.039729	1.439148
207.133586	502.343143	18.960320	-0.039698	1.431492
207.148888	494.533768	18.965325	-0.039696	1.423777
206.894988	486.780696	18.970330	-0.039644	1.416032
206.934278	478.973878	18.975335	-0.039646	1.408240
206.944474	471.178508	18.980339	-0.039643	1.400410
206.961755	463.398764	18.985344	-0.039641	1.392554
206.835980	455.615141	18.990349	-0.039613	1.384624
206.602155	447.878722	18.995354	-0.039565	1.376679
206.766527	440.076180	19.000359	-0.039591	1.368688
206.675561	432.309914	19.005363	-0.039569	1.360644
206.781740	424.546640	19.010368	-0.039584	1.352589
206.455058	416.835578	19.015373	-0.039518	1.344465
206.376864	409.084265	19.020378	-0.039499	1.336292
206.434537	401.317395	19.025383	-0.039505	1.328077
206.492497	393.562012	19.030387	-0.039511	1.319823
206.248534	385.802751	19.035392	-0.039461	1.311459
206.165126	378.006742	19.040397	-0.039440	1.303030
205.961257	370.312111	19.045402	-0.039397	1.294635
205.976926	362.577270	19.050407	-0.039396	1.286181
205.696711	354.902593	19.055411	-0.039339	1.277682
205.658934	347.186782	19.060416	-0.039327	1.269127
205.985725	339.417229	19.065421	-0.039383	1.260522
205.756328	331.759534	19.070426	-0.039335	1.251878
205.851389	324.043918	19.075431	-0.039348	1.243170
205.506406	316.400795	19.080435	-0.039279	1.234399
205.474579	308.691755	19.085440	-0.039269	1.225550
205.285171	301.038413	19.090445	-0.039229	1.216670
205.178908	293.361158	19.095450	-0.039204	1.207713
205.306030	285.677214	19.100455	-0.039223	1.198728
204.938342	278.057493	19.105459	-0.039150	1.189652
205.021570	270.380992	19.110464	-0.039161	1.180530
205.016949	262.720844	19.115469	-0.039155	1.171338
204.951082	255.085348	19.120474	-0.039138	1.162091
204.534728	247.511289	19.125479	-0.039056	1.152771
204.369861	239.852266	19.130483	-0.039020	1.143324
204.585993	232.190729	19.135488	-0.039056	1.133876
204.339008	224.602483	19.140493	-0.039005	1.124341
204.312664	217.003855	19.145498	-0.038995	1.114759
204.167776	209.422550	19.150503	-0.038964	1.105090
204.106170	201.830812	19.155507	-0.038948	1.095341
204.190008	194.226991	19.160512	-0.038958	1.085520
204.155237	186.670551	19.165517	-0.038947	1.075646
204.024723	179.110646	19.170522	-0.038918	1.065654
203.887019	171.583916	19.175527	-0.038888	1.055609
203.834133	164.030899	19.180531	-0.038873	1.045452
203.814583	156.515579	19.185536	-0.038865	1.035255
203.482702	149.043677	19.190541	-0.038799	1.024942
203.337552	141.552336	19.195546	-0.038767	1.014542
203.311961	134.056498	19.200551	-0.038758	1.004056
203.041307	126.602825	19.205555	-0.038703	0.993460
203.095327	119.089801	19.210560	-0.038708	0.982745
202.917643	111.653491	19.215565	-0.038670	0.971964
202.726047	104.232241	19.220570	-0.038630	0.961081
202.941552	96.772087	19.225575	-0.038666	0.950122
202.823189	89.366991	19.230579	-0.038639	0.939029
202.842559	81.967133	19.235584	-0.038638	0.927848
202.678191	74.618365	19.240589	-0.038603	0.916560
202.446424	67.278261	19.245594	-0.038555	0.905127
202.482150	60.156603	19.250599	-0.038557	0.893965