Thu Mar 11 19:06:17 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.577648	-0.077168	0.000000	-0.000073	0.724882

0.462583	-0.052898	0.005005	-0.000052	0.724890
0.526140	-0.071878	0.010010	-0.000064	0.724875
0.565086	-0.219620	0.015014	-0.000072	0.724600
0.634108	-0.236619	0.020019	-0.000085	0.724591
0.601173	-0.230322	0.025024	-0.000079	0.724593
0.642081	-0.235138	0.030029	-0.000087	0.724598
0.676250	-0.246849	0.035034	-0.000093	0.724587
0.579028	-0.223763	0.040038	-0.000076	0.724599
0.600663	-0.231050	0.045043	-0.000080	0.724593
0.764923	-0.261255	0.050048	-0.000111	0.724591
0.622480	-0.233748	0.055053	-0.000084	0.724596
0.425800	-0.203404	0.060058	-0.000048	0.724587
0.487270	-0.275682	0.065062	-0.000060	0.724468
0.529652	-0.393864	0.070067	-0.000068	0.724252
0.535366	-0.392973	0.075072	-0.000069	0.724256
0.633555	-0.406632	0.080077	-0.000088	0.724264
0.659681	-0.416511	0.085082	-0.000093	0.724254
0.485917	-0.382073	0.090086	-0.000061	0.724262
0.496862	-0.404953	0.095091	-0.000063	0.724221
0.683588	-0.578839	0.100096	-0.000098	0.723946
0.420096	-0.527949	0.105101	-0.000049	0.723954
0.284221	-0.508505	0.110106	-0.000024	0.723945
0.499810	-0.543227	0.115110	-0.000064	0.723953
0.542762	-0.578133	0.120115	-0.000073	0.723900
0.575188	-0.724366	0.125120	-0.000079	0.723625
0.374777	-0.686101	0.130125	-0.000042	0.723631
0.476765	-0.708367	0.135130	-0.000061	0.723623
0.587619	-0.723330	0.140134	-0.000082	0.723633
0.626309	-0.880580	0.145139	-0.000089	0.723339
0.639319	-0.882425	0.150144	-0.000092	0.723340
0.458910	-0.849991	0.155149	-0.000059	0.723342
0.441772	-0.910916	0.160154	-0.000056	0.723217
0.794891	-1.081806	0.165158	-0.000122	0.723005
0.647231	-1.058147	0.170163	-0.000094	0.723001
0.632782	-1.076829	0.175168	-0.000092	0.722959
0.562855	-1.200599	0.180173	-0.000079	0.722693
0.428479	-1.180140	0.185178	-0.000054	0.722686
0.710935	-1.242648	0.190182	-0.000107	0.722663
0.732286	-1.396452	0.195187	-0.000111	0.722369
0.685748	-1.388251	0.200192	-0.000103	0.722369
0.605751	-1.419532	0.205197	-0.000088	0.722280
0.360246	-1.484332	0.210202	-0.000043	0.722068
0.394641	-1.487323	0.215206	-0.000049	0.722074
0.569289	-1.618879	0.220211	-0.000082	0.721877
0.521106	-1.679588	0.225216	-0.000073	0.721742
0.532856	-1.688360	0.230221	-0.000076	0.721729
0.624233	-1.855630	0.235226	-0.000093	0.721433
0.598217	-1.847152	0.240230	-0.000088	0.721441
0.500362	-1.940775	0.245235	-0.000070	0.721223
0.354646	-1.969846	0.250240	-0.000043	0.721115
0.506347	-2.034806	0.255245	-0.000072	0.721041
0.404093	-2.102708	0.260250	-0.000053	0.720872
0.431586	-2.119513	0.265254	-0.000058	0.720849
0.463558	-2.284587	0.270259	-0.000064	0.720536
0.445361	-2.279489	0.275264	-0.000061	0.720540
0.330564	-2.409360	0.280269	-0.000040	0.720245
0.271426	-2.412907	0.285274	-0.000029	0.720218
0.359279	-2.561998	0.290278	-0.000046	0.719955
0.041852	-2.534796	0.295283	0.000013	0.719898
-0.177188	-2.610320	0.300288	0.000053	0.719673
0.198423	-2.711520	0.305293	-0.000017	0.719606
-0.252154	-2.756095	0.310298	0.000067	0.719360
-4.479493	-2.050342	0.315302	0.000853	0.719268
-5.077934	-1.945273	0.320307	0.000965	0.719265
-6.161561	-1.751499	0.325312	0.001166	0.719267
-4.830774	-2.076493	0.330317	0.000918	0.719094
-6.540602	-1.843875	0.335322	0.001236	0.718953
-6.751624	-1.801789	0.340326	0.001275	0.718962
-5.883954	-1.959691	0.345331	0.001113	0.718956
-6.449355	-1.859515	0.350336	0.001218	0.718956
-6.724156	-1.808365	0.355341	0.001269	0.718960
-6.560636	-1.841491	0.360346	0.001239	0.718953
-6.315161	-1.965995	0.365350	0.001193	0.718794
-7.199833	-1.888765	0.370355	0.001357	0.718636
-7.141936	-1.899123	0.375360	0.001346	0.718636
-7.084010	-1.906284	0.380365	0.001335	0.718643
-7.417326	-1.851118	0.385370	0.001397	0.718635
-7.196045	-1.887135	0.390374	0.001355	0.718643
-7.213423	-1.885036	0.395379	0.001358	0.718641
-7.836373	-1.905120	0.400384	0.001474	0.718383
-7.969622	-1.897009	0.405389	0.001499	0.718353
-7.942646	-1.906129	0.410394	0.001493	0.718344
-7.879048	-1.913353	0.415398	0.001481	0.718353
-8.352935	-1.831843	0.420403	0.001569	0.718348
-8.355545	-1.832176	0.425408	0.001569	0.718347
-7.827947	-1.925204	0.430413	0.001471	0.718349
-8.906356	-1.906740	0.435418	0.001671	0.718007
-9.111272	-1.865035	0.440422	0.001709	0.718017
-9.091213	-1.871301	0.445427	0.001705	0.718013
-9.170759	-1.858326	0.450432	0.001720	0.718011
-9.202088	-1.849435	0.455437	0.001725	0.718018
-9.265536	-1.842725	0.460442	0.001737	0.718009
-8.866516	-1.909496	0.465446	0.001663	0.718018
-9.348830	-1.925792	0.470451	0.001752	0.717817
-10.739199	-1.741699	0.475456	0.002011	0.717692
-10.032408	-1.861792	0.480461	0.001879	0.717704
-10.145822	-1.846535	0.485466	0.001900	0.717694
-10.358142	-1.805250	0.490470	0.001939	0.717702
-10.118880	-1.849454	0.495475	0.001894	0.717699
-9.917973	-1.885839	0.500480	0.001857	0.717698
-10.136970	-1.844430	0.505485	0.001897	0.717703
-10.648921	-1.904941	0.510490	0.001992	0.717404
-11.161606	-1.827523	0.515494	0.002087	0.717377
-11.482244	-1.772629	0.520499	0.002147	0.717373
-11.352970	-1.795979	0.525504	0.002122	0.717373
-10.791704	-1.890789	0.530509	0.002018	0.717384
-11.279469	-1.809442	0.535514	0.002108	0.717373
-11.288344	-1.805975	0.540518	0.002110	0.717377
-11.268574	-1.811872	0.545523	0.002106	0.717373
-11.576514	-1.900557	0.550528	0.002163	0.717090
-11.985410	-1.832031	0.555533	0.002239	0.717082
-12.496475	-1.743137	0.560538	0.002333	0.717078
-11.510187	-1.916459	0.565542	0.002150	0.717083
-11.498891	-1.919071	0.570547	0.002147	0.717082
-12.124553	-1.809882	0.575552	0.002263	0.717078
-11.725381	-1.876060	0.580557	0.002189	0.717089
-12.447081	-1.909835	0.585562	0.002323	0.716768
-13.092504	-1.800357	0.590566	0.002443	0.716758
-12.932933	-1.830840	0.595571	0.002413	0.716754
-12.737253	-1.867005	0.600576	0.002376	0.716752
-12.859291	-1.842199	0.605581	0.002399	0.716758
-13.279437	-1.771666	0.610586	0.002477	0.716750
-12.875484	-1.840474	0.615590	0.002401	0.716757
-13.051730	-1.872732	0.620595	0.002434	0.716632
-14.242240	-1.755407	0.625600	0.002655	0.716445
-13.531035	-1.880014	0.630605	0.002523	0.716449
-13.943194	-1.810861	0.635610	0.002599	0.716441
-14.023898	-1.791763	0.640614	0.002614	0.716451
-13.921539	-1.815129	0.645619	0.002595	0.716441
-13.877731	-1.820615	0.650624	0.002586	0.716446
-13.862984	-1.821910	0.655629	0.002583	0.716450
-14.571940	-1.831752	0.660634	0.002715	0.716180
-15.051021	-1.770730	0.665638	0.002804	0.716133
-15.010076	-1.779765	0.670643	0.002796	0.716130
-14.869985	-1.806659	0.675648	0.002770	0.716126
-14.842704	-1.808572	0.680653	0.002764	0.716133
-15.041977	-1.778520	0.685658	0.002801	0.716122
-14.540847	-1.865433	0.690662	0.002708	0.716128
-14.765823	-1.843016	0.695667	0.002749	0.716093
-15.611361	-1.799428	0.700672	0.002906	0.715882
-15.230373	-1.864036	0.705677	0.002835	0.715888
-16.071759	-1.719203	0.710682	0.002992	0.715879
-15.409791	-1.834258	0.715686	0.002868	0.715885
-15.332412	-1.851201	0.720691	0.002853	0.715879
-15.942656	-1.745692	0.725696	0.002967	0.715873
-15.437977	-1.868921	0.730701	0.002873	0.715808
-16.402148	-1.832694	0.735706	0.003052	0.715540
-16.508094	-1.810640	0.740710	0.003071	0.715547
-16.793245	-1.763709	0.745715	0.003124	0.715539
-16.488616	-1.817748	0.750720	0.003067	0.715540
-15.812067	-1.936233	0.755725	0.002941	0.715545
-16.509770	-1.815965	0.760730	0.003071	0.715537
-16.702913	-1.831557	0.765734	0.003106	0.715439
-17.417276	-1.813314	0.770739	0.003239	0.715223
-17.313343	-1.830933	0.775744	0.003219	0.715225
-17.505507	-1.792970	0.780749	0.003255	0.715233
-17.529670	-1.792136	0.785754	0.003259	0.715227
-17.389229	-1.815197	0.790758	0.003233	0.715231
-17.410026	-1.815002	0.795763	0.003236	0.715225
-17.560152	-1.793932	0.800768	0.003264	0.715214
-17.642300	-1.933708	0.805773	0.003279	0.714908
-18.482529	-1.788237	0.810778	0.003435	0.714900
-18.272307	-1.822512	0.815782	0.003396	0.714907
-17.819949	-1.904603	0.820787	0.003312	0.714904
-18.587011	-1.769965	0.825792	0.003454	0.714901
-18.415534	-1.796157	0.830797	0.003422	0.714910
-18.219668	-1.849071	0.835802	0.003385	0.714875
-18.978056	-1.848994	0.840806	0.003526	0.714607
-19.445637	-1.766173	0.845811	0.003613	0.714607
-19.295020	-1.794430	0.850816	0.003585	0.714604
-18.681433	-1.901236	0.855821	0.003470	0.714610
-19.405509	-1.777004	0.860826	0.003605	0.714601
-19.450965	-1.766635	0.865830	0.003613	0.714606
-18.916054	-1.861548	0.870835	0.003513	0.714607
-19.641201	-1.893547	0.875840	0.003648	0.714287
-19.983519	-1.835712	0.880845	0.003711	0.714282
-20.459020	-1.755250	0.885850	0.003799	0.714274
-19.768601	-1.876652	0.890854	0.003671	0.714277
-20.013287	-1.834051	0.895859	0.003716	0.714276
-20.297392	-1.785684	0.900864	0.003769	0.714272
-19.691637	-1.889880	0.905869	0.003656	0.714280
-20.682603	-1.869414	0.910874	0.003840	0.713970
-21.143781	-1.788593	0.915878	0.003925	0.713968
-20.950206	-1.824269	0.920883	0.003889	0.713966
-21.221685	-1.779916	0.925888	0.003939	0.713959
-21.218686	-1.775590	0.930893	0.003939	0.713969
-21.140136	-1.793835	0.935898	0.003924	0.713961
-20.949369	-1.825357	0.940902	0.003888	0.713966
-21.166294	-1.853989	0.945907	0.003928	0.713833
-22.247691	-1.758227	0.950912	0.004129	0.713641
-21.385230	-1.906207	0.955917	0.003968	0.713653
-21.980099	-1.804469	0.960922	0.004079	0.713645
-22.400914	-1.727972	0.965926	0.004157	0.713648
-21.894594	-1.816581	0.970931	0.004062	0.713652
-21.894653	-1.820584	0.975936	0.004062	0.713644
-22.066434	-1.807456	0.980941	0.004094	0.713610
-22.778532	-1.811165	0.985946	0.004226	0.713351
-22.749463	-1.813881	0.990950	0.004221	0.713356
-22.914550	-1.784830	0.995955	0.004251	0.713356
-23.016994	-1.767882	1.000960	0.004270	0.713354
-22.738629	-1.814270	1.005965	0.004218	0.713361
-23.006992	-1.770703	1.010970	0.004268	0.713353
-22.921945	-1.783393	1.015974	0.004251	0.713358
-22.809506	-1.923724	1.020979	0.004230	0.713119
-24.195088	-1.728358	1.025984	0.004488	0.713017
-24.128739	-1.735522	1.030989	0.004475	0.713027
-23.768616	-1.804481	1.035994	0.004408	0.713018
-23.800343	-1.797151	1.040998	0.004414	0.713022
-23.762158	-1.803375	1.046003	0.004406	0.713023
-24.269242	-1.717938	1.051008	0.004500	0.713014
-23.811574	-1.820160	1.056013	0.004415	0.712974
-24.362197	-1.860001	1.061018	0.004517	0.712699
-24.573396	-1.819792	1.066022	0.004556	0.712705
-24.825595	-1.773101	1.071027	0.004603	0.712709
-24.542758	-1.827622	1.076032	0.004550	0.712701
-24.505181	-1.828721	1.081037	0.004543	0.712713
-25.132451	-1.723315	1.086042	0.004659	0.712701
-24.730935	-1.801374	1.091046	0.004584	0.712688
-25.153307	-1.879562	1.096051	0.004663	0.712383
-25.786508	-1.768510	1.101056	0.004780	0.712380
-25.499401	-1.814740	1.106061	0.004727	0.712390
-25.710639	-1.782831	1.111066	0.004766	0.712379
-25.667199	-1.787799	1.116070	0.004758	0.712386
-25.782775	-1.768038	1.121075	0.004779	0.712384
-25.402488	-1.839217	1.126080	0.004708	0.712378
-25.770649	-1.893937	1.131085	0.004776	0.712139
-26.821105	-1.735832	1.136090	0.004971	0.712081
-26.165564	-1.849400	1.141094	0.004849	0.712088
-26.261612	-1.833353	1.146099	0.004867	0.712087
-26.963227	-1.711830	1.151104	0.004997	0.712080
-26.442242	-1.799894	1.156109	0.004900	0.712090
-26.298320	-1.829426	1.161114	0.004873	0.712083
-27.038009	-1.832298	1.166118	0.005010	0.711815
-27.705502	-1.742024	1.171123	0.005134	0.711758
-27.298618	-1.817590	1.176128	0.005058	0.711753
-27.364941	-1.800497	1.181133	0.005070	0.711764
-27.960085	-1.699155	1.186138	0.005181	0.711755
-27.436860	-1.790598	1.191142	0.005083	0.711759
-27.313260	-1.814159	1.196147	0.005060	0.711756
-27.537726	-1.813238	1.201152	0.005101	0.711679
-28.235733	-1.802754	1.206157	0.005231	0.711452
-28.229740	-1.807745	1.211162	0.005230	0.711445
-28.505938	-1.755329	1.216166	0.005281	0.711452
-28.260517	-1.800011	1.221171	0.005235	0.711450
-28.213120	-1.810971	1.226176	0.005226	0.711446
-28.336999	-1.785111	1.231181	0.005249	0.711454
-28.330070	-1.806702	1.236186	0.005247	0.711414
-28.853287	-1.852821	1.241190	0.005344	0.711136
-29.142660	-1.800092	1.246195	0.005398	0.711139
-29.890615	-1.670650	1.251200	0.005537	0.711132
-29.119127	-1.803640	1.256205	0.005393	0.711141
-28.918899	-1.843594	1.261210	0.005356	0.711133
-29.242778	-1.783543	1.266214	0.005416	0.711138
-29.462445	-1.745191	1.271219	0.005456	0.711137
-29.489972	-1.853504	1.276224	0.005461	0.710912
-29.875493	-1.804402	1.281229	0.005533	0.710873
-30.244226	-1.743708	1.286234	0.005601	0.710864
-29.908477	-1.800460	1.291238	0.005538	0.710870
-29.829972	-1.815281	1.296243	0.005523	0.710869
-30.135865	-1.763713	1.301248	0.005580	0.710864
-29.900704	-1.818921	1.306253	0.005536	0.710838
-30.709243	-1.832556	1.311258	0.005686	0.710523
-30.935373	-1.792073	1.316262	0.005728	0.710524
-31.058604	-1.766840	1.321267	0.005751	0.710531
-30.981848	-1.783694	1.326272	0.005736	0.710525
-30.920513	-1.789985	1.331277	0.005725	0.710535
-31.306027	-1.726882	1.336282	0.005796	0.710524
-30.963392	-1.786389	1.341286	0.005732	0.710528
-31.185390	-1.879320	1.346291	0.005773	0.710264
-32.408938	-1.689483	1.351296	0.006001	0.710208
-32.191444	-1.725988	1.356301	0.005960	0.710213
-31.530256	-1.846563	1.361306	0.005837	0.710208
-31.922334	-1.774709	1.366310	0.005909	0.710212
-32.135506	-1.735910	1.371315	0.005949	0.710214
-32.034726	-1.756458	1.376320	0.005930	0.710210
-31.604732	-1.908472	1.381325	0.005850	0.710059
-32.741043	-1.791797	1.386330	0.006061	0.709888
-32.471514	-1.839842	1.391334	0.006010	0.709889
-32.441521	-1.843870	1.396339	0.006005	0.709892
-32.734904	-1.796124	1.401344	0.006059	0.709883
-32.637566	-1.807196	1.406349	0.006041	0.709896
-32.967304	-1.756173	1.411354	0.006102	0.709881
-33.181649	-1.834378	1.416358	0.006141	0.709649
-33.594482	-1.788834	1.421363	0.006218	0.709594
-33.745566	-1.766524	1.426368	0.006246	0.709585
-33.546531	-1.797479	1.431373	0.006209	0.709594
-33.846090	-1.748200	1.436378	0.006264	0.709587
-33.783661	-1.756449	1.441382	0.006252	0.709593
-33.371011	-1.829689	1.446387	0.006175	0.709594
-33.938571	-1.835884	1.451392	0.006281	0.709380
-34.896377	-1.721832	1.456397	0.006459	0.709267
-34.406699	-1.814145	1.461402	0.006367	0.709257
-34.273509	-1.838361	1.466406	0.006342	0.709257
-34.714542	-1.759069	1.471411	0.006424	0.709259
-34.633459	-1.775987	1.476416	0.006409	0.709254
-34.187162	-1.851637	1.481421	0.006325	0.709262
-34.474033	-1.884915	1.486426	0.006378	0.709094
-35.886570	-1.703319	1.491430	0.006641	0.708954
-35.233306	-1.818511	1.496435	0.006519	0.708957
-35.478826	-1.779910	1.501440	0.006565	0.708947
-35.554577	-1.762833	1.506445	0.006579	0.708955
-35.270427	-1.817502	1.511450	0.006525	0.708947
-35.287456	-1.812217	1.516454	0.006528	0.708952
-35.454082	-1.849502	1.521459	0.006559	0.708819
-36.438217	-1.768113	1.526464	0.006742	0.708631
-36.139648	-1.818922	1.531469	0.006686	0.708636
-36.564633	-1.745604	1.536474	0.006765	0.708632
-36.345750	-1.782289	1.541478	0.006724	0.708637
-35.991045	-1.847077	1.546483	0.006658	0.708634
-36.487416	-1.762829	1.551488	0.006750	0.708626
-36.638470	-1.755478	1.556493	0.006778	0.708588
-37.148485	-1.786992	1.561498	0.006873	0.708343
-36.961195	-1.819449	1.566502	0.006837	0.708345
-37.473234	-1.727614	1.571507	0.006932	0.708347
-37.467088	-1.733434	1.576512	0.006931	0.708338
-37.023055	-1.807756	1.581517	0.006848	0.708348
-37.279091	-1.767080	1.586522	0.006896	0.708339
-37.349528	-1.751771	1.591526	0.006908	0.708345
-37.706181	-1.839464	1.596531	0.006975	0.708042
-38.498783	-1.717904	1.601536	0.007122	0.708003
-38.332212	-1.744918	1.606541	0.007091	0.708009
-38.145387	-1.781226	1.611546	0.007056	0.708003
-38.373799	-1.739864	1.616550	0.007098	0.708005
-38.295026	-1.751813	1.621555	0.007083	0.708010
-38.187078	-1.774101	1.626560	0.007063	0.708004
-37.886831	-1.891625	1.631565	0.007007	0.707876
-38.979270	-1.788767	1.636570	0.007210	0.707693
-38.803039	-1.821474	1.641574	0.007177	0.707690
-38.857341	-1.809705	1.646579	0.007186	0.707695
-39.091129	-1.771470	1.651584	0.007230	0.707689
-39.070300	-1.769591	1.656589	0.007226	0.707700
-39.428495	-1.712255	1.661594	0.007292	0.707688
-39.005170	-1.870517	1.666598	0.007213	0.707522
-39.938125	-1.779271	1.671603	0.007386	0.707372
-40.118559	-1.750699	1.676608	0.007420	0.707365
-39.895181	-1.786131	1.681613	0.007378	0.707375
-40.051725	-1.759756	1.686618	0.007407	0.707372
-40.335601	-1.708313	1.691622	0.007459	0.707374
-40.120416	-1.744657	1.696627	0.007419	0.707379
-40.139045	-1.749244	1.701632	0.007422	0.707363
-40.396939	-1.842770	1.706637	0.007470	0.707084
-40.741108	-1.784855	1.711642	0.007534	0.707078
-40.752459	-1.782066	1.716646	0.007536	0.707080
-40.547075	-1.817754	1.721651	0.007497	0.707082
-40.980591	-1.743602	1.726656	0.007578	0.707076
-40.880579	-1.757941	1.731661	0.007559	0.707084
-40.820171	-1.800793	1.736666	0.007547	0.707020
-41.890757	-1.746547	1.741670	0.007746	0.706746
-41.543841	-1.806999	1.746675	0.007682	0.706749
-41.849777	-1.754653	1.751680	0.007738	0.706745
-41.694566	-1.779805	1.756685	0.007709	0.706751
-41.879119	-1.750534	1.761690	0.007743	0.706744
-41.736787	-1.774323	1.766694	0.007716	0.706748
-41.471646	-1.821636	1.771699	0.007667	0.706748
-42.561750	-1.783312	1.776704	0.007870	0.706435
-42.621132	-1.770408	1.781709	0.007880	0.706440
-42.624546	-1.772375	1.786714	0.007881	0.706436
-42.471530	-1.798187	1.791718	0.007852	0.706439
-42.574616	-1.778347	1.796723	0.007871	0.706443
-42.802635	-1.741752	1.801728	0.007913	0.706435
-42.419792	-1.805891	1.806733	0.007842	0.706444
-43.068992	-1.835373	1.811738	0.007962	0.706152
-43.648783	-1.748337	1.816742	0.008070	0.706120
-43.359405	-1.799429	1.821747	0.008016	0.706121
-43.390149	-1.797687	1.826752	0.008021	0.706114
-43.223445	-1.821826	1.831757	0.007990	0.706126
-43.399898	-1.793993	1.836762	0.008023	0.706119
-43.495863	-1.784702	1.841766	0.008040	0.706104
-44.028536	-1.811635	1.846771	0.008139	0.705860
-44.108455	-1.801398	1.851776	0.008154	0.705852
-44.218571	-1.779878	1.856781	0.008174	0.705856
-44.292835	-1.769562	1.861786	0.008187	0.705851
-44.235520	-1.780063	1.866790	0.008177	0.705851
-44.155406	-1.793580	1.871795	0.008161	0.705853
-44.483410	-1.786963	1.876800	0.008222	0.705749
-45.264199	-1.760329	1.881805	0.008367	0.705523
-44.934742	-1.823339	1.886810	0.008306	0.705515
-45.432774	-1.733172	1.891814	0.008398	0.705518
-45.452339	-1.727679	1.896819	0.008402	0.705523
-45.293430	-1.759666	1.901824	0.008372	0.705516
-44.890693	-1.829262	1.906829	0.008297	0.705521
-45.165541	-1.810686	1.911834	0.008347	0.705460
-46.097931	-1.771203	1.916838	0.008521	0.705205
-45.831613	-1.816289	1.921843	0.008471	0.705211
-46.280276	-1.740776	1.926848	0.008554	0.705202
-45.938053	-1.798424	1.931853	0.008490	0.705210
-45.955694	-1.797889	1.936858	0.008493	0.705205
-46.567652	-1.690279	1.941862	0.008607	0.705202
-46.265870	-1.740369	1.946867	0.008550	0.705210
-46.602922	-1.838864	1.951872	0.008613	0.704891
-46.888539	-1.790709	1.956877	0.008666	0.704886
-47.045440	-1.766043	1.961882	0.008695	0.704880
-46.817123	-1.805248	1.966886	0.008652	0.704884
-46.464570	-1.866058	1.971891	0.008586	0.704888
-47.187364	-1.741554	1.976896	0.008721	0.704880
-47.009375	-1.792672	1.981901	0.008687	0.704841
-47.636331	-1.808797	1.986906	0.008804	0.704584
-47.646370	-1.805858	1.991910	0.008805	0.704587
-48.023095	-1.737120	1.996915	0.008875	0.704591
-47.774867	-1.783452	2.001920	0.008829	0.704587

-48.111816	-1.723947	2.011917	0.008891	0.704587
-47.873993	-1.771722	2.021914	0.008846	0.704577
-48.677743	-1.786882	2.031910	0.008995	0.704259
-48.931931	-1.742053	2.041907	0.009042	0.704259
-48.325644	-1.825901	2.051904	0.008929	0.704308
-48.514194	-1.713602	2.061901	0.008963	0.704468
-47.962267	-1.825285	2.071898	0.008860	0.704442
-48.083322	-1.729814	2.081894	0.008882	0.704592
-47.438682	-1.848060	2.091891	0.008762	0.704586
-48.120066	-1.727499	2.101888	0.008888	0.704586
-47.905592	-1.766186	2.111885	0.008847	0.704586
-47.809942	-1.782137	2.121882	0.008829	0.704589
-47.850774	-1.773873	2.131878	0.008836	0.704592
-47.902885	-1.765653	2.141875	0.008845	0.704591
-47.393381	-1.781649	2.151872	0.008750	0.704742
-47.119100	-1.760853	2.161869	0.008698	0.704884
-46.976235	-1.786773	2.171866	0.008671	0.704884
-47.236669	-1.739320	2.181862	0.008719	0.704887
-46.866605	-1.804851	2.191859	0.008650	0.704889
-46.696707	-1.686600	2.201856	0.008618	0.705189
-46.021966	-1.798177	2.211853	0.008492	0.705207
-46.226312	-1.761460	2.221850	0.008529	0.705209
-46.233246	-1.750038	2.231846	0.008530	0.705231
-45.614715	-1.714213	2.241843	0.008414	0.705526
-45.302704	-1.771566	2.251840	0.008356	0.705523
-45.481252	-1.740304	2.261837	0.008388	0.705523
-45.021195	-1.757397	2.271834	0.008302	0.705654
-44.331076	-1.778849	2.281830	0.008173	0.705860
-44.334717	-1.777057	2.291827	0.008173	0.705863
-44.429982	-1.762662	2.301824	0.008191	0.705859
-44.030762	-1.763318	2.311821	0.008116	0.706002
-43.643906	-1.770696	2.321818	0.008043	0.706126
-43.653069	-1.768113	2.331814	0.008044	0.706129
-43.385613	-1.817134	2.341811	0.007994	0.706128
-43.005898	-1.743396	2.351808	0.007923	0.706413
-42.947447	-1.741160	2.361805	0.007911	0.706439
-42.560641	-1.808422	2.371802	0.007839	0.706444
-42.740479	-1.705443	2.381798	0.007872	0.706587
-41.706511	-1.807765	2.391795	0.007679	0.706753
-41.973997	-1.763609	2.401792	0.007728	0.706747
-41.919590	-1.763836	2.411789	0.007717	0.706767
-41.407907	-1.699938	2.421786	0.007622	0.707079
-40.905299	-1.790173	2.431782	0.007528	0.707079
-41.228556	-1.733041	2.441779	0.007587	0.707079
-40.605867	-1.732667	2.451776	0.007471	0.707303
-40.199545	-1.771702	2.461773	0.007395	0.707371
-40.110882	-1.787099	2.471770	0.007378	0.707373
-40.223389	-1.730029	2.481766	0.007398	0.707448
-39.379608	-1.756764	2.491763	0.007240	0.707697
-39.308293	-1.769652	2.501760	0.007227	0.707698
-39.464758	-1.744552	2.511757	0.007255	0.707693
-38.738507	-1.736259	2.521754	0.007120	0.707971
-38.238831	-1.805539	2.531750	0.007026	0.708011
-38.267208	-1.801477	2.541747	0.007031	0.708010
-38.435153	-1.733049	2.551744	0.007062	0.708088
-37.412740	-1.789509	2.561741	0.006871	0.708342
-37.450774	-1.783336	2.571738	0.006877	0.708341
-37.636562	-1.750049	2.581734	0.006911	0.708343
-36.895109	-1.779439	2.591731	0.006773	0.708549
-36.686420	-1.774792	2.601728	0.006733	0.708634
-36.741983	-1.766822	2.611725	0.006743	0.708631
-36.695280	-1.744888	2.621722	0.006734	0.708693
-35.836438	-1.770006	2.631718	0.006574	0.708950
-35.770493	-1.781389	2.641715	0.006561	0.708952
-35.778856	-1.780387	2.651712	0.006562	0.708952
-35.287670	-1.752229	2.661709	0.006470	0.709184
-35.002837	-1.765094	2.671706	0.006416	0.709261
-34.896633	-1.785839	2.681702	0.006396	0.709259
-34.942512	-1.727535	2.691699	0.006404	0.709360
-33.867499	-1.804329	2.701696	0.006203	0.709591
-34.101950	-1.762762	2.711693	0.006247	0.709591
-33.886006	-1.801696	2.721690	0.006206	0.709591
-33.466028	-1.781409	2.731686	0.006127	0.709782
-33.323592	-1.752014	2.741683	0.006100	0.709893
-33.352745	-1.748910	2.751680	0.006105	0.709890
-33.270501	-1.714057	2.761677	0.006089	0.709990
-32.398514	-1.759639	2.771674	0.005926	0.710210
-32.195135	-1.795043	2.781670	0.005888	0.710213
-32.386737	-1.761347	2.791667	0.005923	0.710213
-31.531626	-1.772505	2.801664	0.005763	0.710496
-31.699918	-1.727862	2.811661	0.005794	0.710526
-31.444101	-1.773470	2.821658	0.005746	0.710527
-31.294554	-1.719452	2.831654	0.005718	0.710689
-30.493401	-1.773037	2.841651	0.005568	0.710868
-30.612694	-1.754069	2.851648	0.005590	0.710865
-30.525775	-1.771221	2.861645	0.005573	0.710862
-29.936393	-1.752389	2.871642	0.005463	0.711111
-29.595564	-1.802178	2.881638	0.005399	0.711133
-29.986546	-1.732838	2.891635	0.005471	0.711134
-29.514317	-1.728648	2.901632	0.005383	0.711311
-29.009128	-1.750368	2.911629	0.005288	0.711448
-28.991656	-1.754401	2.921626	0.005284	0.711447
-28.933728	-1.722426	2.931622	0.005273	0.711533
-28.129932	-1.752806	2.941619	0.005123	0.711759
-28.096334	-1.759438	2.951616	0.005116	0.711758
-27.978293	-1.782803	2.961613	0.005094	0.711755
-27.456603	-1.749974	2.971610	0.004996	0.712006
-26.960771	-1.797679	2.981606	0.004903	0.712088
-27.191753	-1.755951	2.991603	0.004946	0.712090
-27.033147	-1.756935	3.001600	0.004915	0.712146
-26.471017	-1.738417	3.011597	0.004810	0.712383
-26.179711	-1.790850	3.021594	0.004756	0.712383
-26.491579	-1.736123	3.031590	0.004813	0.712382
-25.773516	-1.733650	3.041587	0.004679	0.712643
-25.463811	-1.758825	3.051584	0.004621	0.712704
-25.564833	-1.741628	3.061581	0.004639	0.712703
-25.297647	-1.724128	3.071578	0.004589	0.712834
-24.613279	-1.754244	3.081574	0.004461	0.713018
-24.614551	-1.753563	3.091571	0.004461	0.713019
-24.345837	-1.802637	3.101568	0.004410	0.713018
-23.922513	-1.725207	3.111565	0.004331	0.713323
-23.466675	-1.792454	3.121562	0.004245	0.713352
-23.682914	-1.755123	3.131558	0.004285	0.713350
-23.606840	-1.715728	3.141555	0.004270	0.713457
-22.882444	-1.750292	3.151552	0.004135	0.713646
-22.847123	-1.758961	3.161549	0.004128	0.713642
-22.717000	-1.781965	3.171546	0.004103	0.713643
-22.216658	-1.723146	3.181542	0.004009	0.713938
-21.841145	-1.777560	3.191539	0.003939	0.713964
-21.870068	-1.773289	3.201536	0.003944	0.713963
-21.917420	-1.704462	3.211533	0.003952	0.714084
-20.808779	-1.809120	3.221530	0.003745	0.714270
-21.110786	-1.754663	3.231526	0.003801	0.714272
-21.105949	-1.753968	3.241523	0.003800	0.714276
-20.368258	-1.731545	3.251520	0.003662	0.714583
-20.299160	-1.732969	3.261517	0.003648	0.714605
-20.187070	-1.753073	3.271514	0.003627	0.714606
-20.111128	-1.690131	3.281510	0.003612	0.714759
-19.155769	-1.787464	3.291507	0.003434	0.714904
-19.479467	-1.729892	3.301504	0.003494	0.714905
-19.340940	-1.748365	3.311501	0.003467	0.714918
-18.474313	-1.749588	3.321498	0.003305	0.715223
-18.262610	-1.785506	3.331494	0.003266	0.715228
-18.167731	-1.800967	3.341491	0.003247	0.715232
-18.270125	-1.721197	3.351488	0.003266	0.715355
-17.116492	-1.834033	3.361485	0.003051	0.715539
-17.285599	-1.804081	3.371482	0.003082	0.715540
-17.310150	-1.800551	3.381478	0.003086	0.715539
-16.944708	-1.783830	3.391475	0.003017	0.715702
-16.420453	-1.788913	3.401472	0.002919	0.715878
-16.326744	-1.805977	3.411469	0.002901	0.715879
-16.317712	-1.808074	3.421466	0.002899	0.715879
-16.058173	-1.775838	3.431462	0.002850	0.716035
-15.612317	-1.808177	3.441459	0.002766	0.716129
-15.561835	-1.817698	3.451456	0.002757	0.716129
-15.651978	-1.771356	3.461453	0.002773	0.716190
-14.539774	-1.841916	3.471450	0.002565	0.716444
-14.529454	-1.845072	3.481446	0.002563	0.716442
-14.467427	-1.855070	3.491443	0.002551	0.716445
-14.511199	-1.768856	3.501440	0.002558	0.716601
-13.508025	-1.873419	3.511437	0.002371	0.716749
-13.990017	-1.788762	3.521434	0.002460	0.716748
-13.706843	-1.838783	3.531430	0.002407	0.716750
-13.008152	-1.805748	3.541427	0.002276	0.717062
-12.945152	-1.808886	3.551424	0.002264	0.717079
-12.874810	-1.823405	3.561421	0.002251	0.717076
-12.704039	-1.800187	3.571418	0.002218	0.717183
-11.920754	-1.842234	3.581414	0.002072	0.717377
-11.886327	-1.848143	3.591411	0.002065	0.717378
-12.276692	-1.780049	3.601408	0.002137	0.717376
-11.210227	-1.821148	3.611405	0.001938	0.717672
-11.410026	-1.773396	3.621402	0.001975	0.717697
-10.916092	-1.860320	3.631398	0.001882	0.717700
-11.100481	-1.763470	3.641395	0.001916	0.717827
-10.075728	-1.850682	3.651392	0.001725	0.718016
-10.239416	-1.823242	3.661389	0.001755	0.718014
-10.391731	-1.795534	3.671386	0.001783	0.718016
-9.493282	-1.806084	3.681382	0.001615	0.718312
-9.249754	-1.830277	3.691379	0.001569	0.718351
-9.251019	-1.829235	3.701376	0.001569	0.718354
-9.240401	-1.808539	3.711373	0.001566	0.718399
-8.540543	-1.811904	3.721370	0.001435	0.718640
-8.262058	-1.861319	3.731366	0.001383	0.718641
-8.662367	-1.789600	3.741363	0.001457	0.718643
-7.980894	-1.794477	3.751360	0.001330	0.718874
-7.777139	-1.789544	3.761357	0.001291	0.718956
-7.433076	-1.851826	3.771354	0.001227	0.718955
-7.519257	-1.803253	3.781350	0.001242	0.719021
-6.554167	-1.850687	3.791347	0.001062	0.719268
-6.467283	-1.868749	3.801344	0.001045	0.719264
-6.618096	-1.842933	3.811341	0.001073	0.719263
-6.526831	-1.777789	3.821338	0.001055	0.719424
-5.612123	-1.853525	3.831334	0.000885	0.719597
-5.919724	-1.798320	3.841331	0.000941	0.719599
-5.529624	-1.868480	3.851328	0.000868	0.719598
-5.142764	-1.794895	3.861325	0.000796	0.719880
-4.767951	-1.854121	3.871322	0.000725	0.719896
-4.850965	-1.839667	3.881318	0.000740	0.719896
-4.691121	-1.797094	3.891315	0.000710	0.720037
-3.870518	-1.850032	3.901312	0.000557	0.720222
-4.032359	-1.823406	3.911309	0.000586	0.720218
-3.989766	-1.831361	3.921306	0.000578	0.720218
-3.298562	-1.809936	3.931302	0.000449	0.720504
-3.318533	-1.788446	3.941299	0.000452	0.720540
-3.113993	-1.825240	3.951296	0.000413	0.720540
-2.937127	-1.789600	3.961293	0.000380	0.720674
-2.290222	-1.803371	3.971290	0.000259	0.720874
-2.163941	-1.823765	3.981286	0.000235	0.720879
-2.225791	-1.812365	3.991283	0.000246	0.720881
-1.723310	-1.792636	4.001280	0.000152	0.721097
-1.640660	-1.795841	4.011277	0.000136	0.721120
-1.441024	-1.832714	4.021274	0.000098	0.721119
-1.445469	-1.734125	4.031270	0.000098	0.721312
-1.428262	-1.672086	4.041267	0.000095	0.721441
-1.064567	-1.738331	4.051264	0.000026	0.721439
-1.239055	-1.578200	4.061261	0.000058	0.721693
-1.210885	-1.559324	4.071258	0.000053	0.721741
-1.002423	-1.508944	4.081254	0.000013	0.721914
-0.791467	-1.465272	4.091251	-0.000027	0.722075
-0.932652	-1.384192	4.101248	-0.000001	0.722186
-0.757578	-1.324069	4.111245	-0.000034	0.722366
-0.748277	-1.247067	4.121242	-0.000036	0.722521
-0.512558	-1.203393	4.131238	-0.000081	0.722690
-0.719215	-1.058784	4.141235	-0.000043	0.722903
-0.720848	-0.992208	4.151232	-0.000043	0.723034
-0.697568	-0.841254	4.161229	-0.000048	0.723339
-0.806465	-0.732217	4.171226	-0.000028	0.723515
-0.457265	-0.702564	4.181222	-0.000094	0.723696
-0.500092	-0.564952	4.191219	-0.000087	0.723952
-0.439431	-0.441329	4.201216	-0.000098	0.724216
-0.266472	-0.355654	4.211213	-0.000131	0.724445
-0.211351	-0.247286	4.221210	-0.000142	0.724677
-0.170361	-0.135484	4.231206	-0.000150	0.724911
-0.338435	0.048942	4.241203	-0.000120	0.725215
0.000000	0.160810	4.251200	-0.000183	0.725552

0.073527	0.756076	4.256205	-0.000198	0.726741
0.144118	2.017114	4.261210	-0.000212	0.729222
0.281137	3.861405	4.266214	-0.000239	0.732847
0.336181	6.265314	4.271219	-0.000251	0.737504
0.725132	9.122052	4.276224	-0.000325	0.743109
1.321920	12.435903	4.281229	-0.000439	0.749607
1.318800	16.295908	4.286234	-0.000441	0.756873
1.737210	20.494702	4.291238	-0.000522	0.764838
1.953727	25.130270	4.296243	-0.000566	0.773456
2.448230	30.074114	4.301248	-0.000661	0.782626
2.712217	35.419182	4.306253	-0.000714	0.792336
3.010187	41.056268	4.311258	-0.000773	0.802455
3.669263	46.947435	4.316262	-0.000900	0.813002
4.194714	53.140595	4.321267	-0.001002	0.823893
4.469773	59.657483	4.326272	-0.001058	0.835116
5.367819	66.284145	4.331277	-0.001230	0.846558
5.895385	73.201995	4.336282	-0.001333	0.858221
6.452810	80.327795	4.341286	-0.001442	0.870074
6.811439	87.654472	4.346291	-0.001513	0.882035
7.572916	95.098171	4.351296	-0.001660	0.894133
8.815082	102.610713	4.356301	-0.001897	0.906309
9.396564	110.399806	4.361306	-0.002010	0.918571
10.144468	118.270697	4.366310	-0.002155	0.930839
10.945501	126.247232	4.371315	-0.002310	0.943121
11.625796	134.360844	4.376320	-0.002442	0.955416
12.338008	142.546288	4.381325	-0.002580	0.967668
13.287485	150.776757	4.386330	-0.002762	0.979892
14.165386	159.138049	4.391334	-0.002932	0.992133
15.270987	167.474804	4.396339	-0.003143	1.004246
15.640840	175.995946	4.401344	-0.003218	1.016293
16.465704	184.472630	4.406349	-0.003377	1.028246
17.576692	192.936731	4.411354	-0.003590	1.040111
18.480290	201.483361	4.416358	-0.003764	1.051905
18.887673	210.135293	4.421363	-0.003846	1.063594
19.471763	218.787388	4.426368	-0.003960	1.075196
20.255388	227.396708	4.431373	-0.004112	1.086662
20.744584	236.063143	4.436378	-0.004209	1.098017
21.717267	244.654689	4.441382	-0.004396	1.109266
22.451126	253.285223	4.446387	-0.004539	1.120399
23.111810	261.930097	4.451392	-0.004667	1.131424
23.817574	270.573904	4.456397	-0.004805	1.142350
24.218318	279.285128	4.461402	-0.004885	1.153191
25.120155	287.868020	4.466406	-0.005059	1.163880
25.756490	296.492452	4.471411	-0.005183	1.174465
26.184993	305.126090	4.476416	-0.005269	1.184925
26.822283	313.738748	4.481421	-0.005394	1.195310
27.601139	322.278272	4.486426	-0.005544	1.205548
28.118460	330.890069	4.491430	-0.005647	1.215731
28.534383	339.476829	4.496435	-0.005730	1.225781
29.308399	348.021868	4.501440	-0.005880	1.235771
30.349126	356.490620	4.506445	-0.006079	1.245645
30.988227	365.019981	4.511450	-0.006204	1.255432
31.537556	373.557818	4.516454	-0.006312	1.265136
31.944363	382.107396	4.521459	-0.006394	1.274752
32.432540	390.608248	4.526464	-0.006491	1.284257
32.993709	399.106278	4.531469	-0.006601	1.293702
33.600998	407.560855	4.536474	-0.006720	1.303040
33.943383	416.155754	4.541478	-0.006789	1.312415
34.334238	424.633902	4.546483	-0.006868	1.321606
34.892018	433.028735	4.551488	-0.006978	1.330675
35.595938	441.409743	4.556493	-0.007114	1.339694
35.662002	449.867257	4.561498	-0.007132	1.348620
36.194437	458.258150	4.566502	-0.007237	1.357500
36.791047	466.603301	4.571507	-0.007354	1.366285
37.284463	474.988236	4.576512	-0.007452	1.375036
37.585479	483.385179	4.581517	-0.007513	1.383712
38.181083	491.737082	4.586522	-0.007630	1.392338
38.747727	500.075243	4.591526	-0.007741	1.400891
39.038774	508.440426	4.596531	-0.007801	1.409374
39.566647	516.767522	4.601536	-0.007905	1.417807
40.011863	525.090335	4.606541	-0.007994	1.426172
40.448560	533.424780	4.611546	-0.008081	1.434498
41.092311	541.701573	4.616550	-0.008206	1.442753
41.427205	550.037603	4.621555	-0.008274	1.450968
41.987278	558.317201	4.626560	-0.008384	1.459119
42.558345	566.612700	4.631565	-0.008496	1.467241
43.113881	574.944229	4.636570	-0.008605	1.475350
43.443079	583.237539	4.641574	-0.008672	1.483343
43.825190	591.524709	4.646579	-0.008749	1.491295
44.443025	599.769601	4.651584	-0.008870	1.499201
44.731948	608.072864	4.656589	-0.008929	1.507070
45.038873	616.361942	4.661594	-0.008992	1.514888
45.556395	624.598098	4.666598	-0.009094	1.522648
45.991687	632.849035	4.671603	-0.009181	1.530370
46.183198	641.141156	4.676608	-0.009222	1.538054
46.751278	649.359129	4.681613	-0.009333	1.545688
46.952575	657.654616	4.686618	-0.009376	1.553300
47.616257	665.835627	4.691622	-0.009506	1.560840
48.079519	674.057801	4.696627	-0.009598	1.568351
48.505297	682.290275	4.701632	-0.009682	1.575829
49.138875	690.488967	4.706637	-0.009806	1.583272
49.270348	698.762636	4.711642	-0.009836	1.590675
49.564557	707.007506	4.716646	-0.009897	1.598041
50.128358	715.176570	4.721651	-0.010007	1.605345
50.395571	723.429681	4.726656	-0.010062	1.612647
50.818250	731.636379	4.731661	-0.010147	1.619897
51.494944	739.793645	4.736666	-0.010278	1.627108
52.198194	748.036806	4.741670	-0.010415	1.634364
52.702442	756.201547	4.746675	-0.010514	1.641493
53.488376	764.339319	4.751680	-0.010666	1.648606
54.037875	772.535454	4.756685	-0.010774	1.655706
54.340089	780.744780	4.761690	-0.010836	1.662754
54.667489	788.966170	4.766694	-0.010903	1.669785
55.231889	797.145475	4.771699	-0.011013	1.676783
55.623954	805.321557	4.776704	-0.011092	1.683726
55.866878	813.555814	4.781709	-0.011143	1.690669
56.199332	821.753563	4.786714	-0.011210	1.697565
56.814395	829.896668	4.791718	-0.011330	1.704425
57.275178	838.091915	4.796723	-0.011422	1.711280
57.605261	846.282018	4.801728	-0.011489	1.718086
58.232188	854.422571	4.806733	-0.011611	1.724863
58.448184	862.618333	4.811738	-0.011657	1.731605
58.839249	870.799688	4.816742	-0.011735	1.738332
59.268959	878.935165	4.821747	-0.011821	1.745001
60.017382	887.056637	4.826752	-0.011966	1.751673
60.273557	895.258830	4.831757	-0.012019	1.758323
60.542224	903.402464	4.836762	-0.012075	1.764902
60.848312	911.595762	4.841766	-0.012137	1.771500
61.154916	919.768701	4.846771	-0.012200	1.778058
61.541065	927.898794	4.851776	-0.012277	1.784568
62.322901	936.045163	4.856781	-0.012429	1.791115
62.654100	944.221821	4.861786	-0.012496	1.797608
62.790132	952.382022	4.866790	-0.012527	1.804039
63.203902	960.515193	4.871795	-0.012609	1.810461
63.477958	968.681812	4.876800	-0.012666	1.816869
63.618427	976.841263	4.881805	-0.012698	1.823233
63.740417	985.003385	4.886810	-0.012726	1.829574
64.419763	993.107429	4.891814	-0.012858	1.835915
64.694258	1001.238158	4.896819	-0.012915	1.842206
65.040878	1009.366946	4.901824	-0.012985	1.848483
65.647485	1017.487763	4.906829	-0.013103	1.854763
65.855516	1025.635299	4.911834	-0.013148	1.860996
66.100780	1033.790472	4.916838	-0.013199	1.867217
66.585542	1041.928898	4.921843	-0.013295	1.873433
66.896679	1050.045843	4.926848	-0.013358	1.879592
67.228744	1058.163659	4.931853	-0.013425	1.885734
67.489195	1066.306221	4.936858	-0.013480	1.891866
67.751043	1074.453902	4.941862	-0.013534	1.897983
68.268817	1082.537451	4.946867	-0.013636	1.904060
68.161255	1090.728327	4.951872	-0.013621	1.910128
68.632771	1098.839632	4.956877	-0.013715	1.916182
68.974486	1106.930712	4.961882	-0.013784	1.922188
69.043834	1115.091699	4.966886	-0.013802	1.928196
69.448282	1123.193824	4.971891	-0.013883	1.934180
70.009059	1131.274140	4.976896	-0.013993	1.940146
70.509780	1139.385426	4.981901	-0.014092	1.946109
70.816261	1147.550552	4.986906	-0.014155	1.952072
71.002968	1155.691941	4.991910	-0.014195	1.957987
71.622695	1163.733755	4.996915	-0.014316	1.963859
71.760312	1171.863995	5.001920	-0.014347	1.969724
72.054831	1179.984947	5.006925	-0.014407	1.975583
72.463990	1188.054836	5.011930	-0.014489	1.981400
72.690876	1196.179887	5.016934	-0.014537	1.987219
73.064379	1204.298374	5.021939	-0.014612	1.993032
73.349540	1212.403973	5.026944	-0.014671	1.998810
73.620642	1220.503089	5.031949	-0.014727	2.004565
74.015175	1228.593475	5.036954	-0.014806	2.010311
74.399422	1236.713098	5.041958	-0.014883	2.016059
75.037324	1244.767920	5.046963	-0.015007	2.021772
75.246961	1252.885086	5.051968	-0.015051	2.027467
75.451239	1261.064184	5.056973	-0.015095	2.033190
75.810049	1269.140103	5.061978	-0.015167	2.038840
76.230100	1277.215304	5.066982	-0.015251	2.044480
76.345732	1285.346972	5.071987	-0.015278	2.050113
76.738295	1293.440813	5.076992	-0.015357	2.055733
77.103089	1301.538004	5.081997	-0.015430	2.061336
77.286284	1309.634828	5.087002	-0.015470	2.066906
77.672154	1317.752883	5.092006	-0.015547	2.072495
77.986546	1325.839641	5.097011	-0.015611	2.078041
78.261093	1333.908788	5.102016	-0.015668	2.083556
78.879809	1341.983169	5.107021	-0.015789	2.089093
79.037189	1350.107160	5.112026	-0.015824	2.094605
79.512068	1358.187670	5.117030	-0.015918	2.100103
79.926860	1366.270337	5.122035	-0.016000	2.105583
80.056936	1374.419980	5.127040	-0.016030	2.111065
80.432568	1382.557115	5.132045	-0.016106	2.116549
80.751262	1390.591606	5.137050	-0.016170	2.121944
81.101730	1398.665232	5.142054	-0.016241	2.127355
81.556007	1406.757947	5.147059	-0.016331	2.132775
81.707188	1414.858516	5.152064	-0.016365	2.138157
82.298580	1422.915563	5.157069	-0.016481	2.143538
82.483546	1431.011686	5.162074	-0.016521	2.148893
82.834526	1439.127953	5.167078	-0.016592	2.154264
82.743981	1447.245364	5.172083	-0.016580	2.159580
82.972806	1455.303272	5.177088	-0.016628	2.164875
83.397608	1463.388859	5.182093	-0.016713	2.170193
83.761182	1471.456755	5.187098	-0.016786	2.175480
84.052801	1479.534332	5.192102	-0.016846	2.180754
84.662383	1487.572374	5.197107	-0.016965	2.186019
84.663253	1495.724682	5.202112	-0.016971	2.191289
85.039915	1503.814166	5.207117	-0.017046	2.196541
85.310289	1511.863247	5.212122	-0.017102	2.201744
85.815199	1519.909705	5.217126	-0.017202	2.206954
85.911929	1528.037439	5.222131	-0.017225	2.212167
86.234721	1536.110314	5.227136	-0.017291	2.217353
86.555212	1544.185496	5.232141	-0.017356	2.222529
86.938910	1552.237207	5.237146	-0.017433	2.227682
87.126491	1560.366363	5.242150	-0.017474	2.232856
87.463206	1568.439586	5.247155	-0.017542	2.237995
87.631046	1576.498034	5.252160	-0.017579	2.243098
88.111829	1584.562581	5.257165	-0.017674	2.248221
88.244319	1592.675735	5.262170	-0.017704	2.253333
88.701554	1600.724131	5.267174	-0.017794	2.258420
88.817355	1608.818946	5.272179	-0.017822	2.263495
89.013027	1616.908181	5.277184	-0.017863	2.268562
89.564358	1625.032137	5.282189	-0.017972	2.273670
89.788268	1633.087025	5.287194	-0.018019	2.278696
89.971186	1641.144862	5.292198	-0.018058	2.283708
90.422641	1649.175686	5.297203	-0.018148	2.288716
90.830828	1657.234940	5.302208	-0.018230	2.293727
91.205814	1665.296386	5.307213	-0.018305	2.298725
91.341611	1673.373919	5.312218	-0.018336	2.303702
91.658579	1681.449027	5.317222	-0.018400	2.308682
92.061696	1689.527199	5.322227	-0.018481	2.313660
92.278146	1697.583847	5.327232	-0.018527	2.318599
92.539143	1705.669701	5.332237	-0.018581	2.323548
92.963272	1713.704239	5.337242	-0.018665	2.328470
93.370025	1721.789602	5.342246	-0.018746	2.333410
93.743719	1729.861014	5.347251	-0.018822	2.338329
93.917078	1737.931108	5.352256	-0.018859	2.343220
94.121967	1746.036724	5.357261	-0.018903	2.348124
94.256804	1754.138019	5.362266	-0.018934	2.353010
94.627295	1762.175747	5.367270	-0.019008	2.357867
94.941493	1770.233734	5.372275	-0.019072	2.362722
95.279169	1778.271908	5.377280	-0.019141	2.367556
95.736053	1786.351291	5.382285	-0.019231	2.372415
95.970417	1794.409763	5.387290	-0.019280	2.377233
96.179906	1802.477312	5.392294	-0.019325	2.382045
96.385819	1810.548632	5.397299	-0.019369	2.386849
96.489444	1818.637905	5.402304	-0.019393	2.391646
96.792704	1826.716566	5.407309	-0.019455	2.396443
97.175327	1834.732931	5.412314	-0.019532	2.401199
97.494335	1842.790125	5.417318	-0.019597	2.405966
97.755643	1850.865604	5.422323	-0.019651	2.410729
97.786569	1858.969435	5.427328	-0.019663	2.415481
98.123846	1867.018450	5.432333	-0.019731	2.420215
98.175744	1875.093943	5.437338	-0.019746	2.424934
98.469932	1883.161758	5.442342	-0.019806	2.429657
98.998245	1891.278788	5.447347	-0.019910	2.434418
99.287218	1899.277773	5.452352	-0.019969	2.439083
99.497479	1907.330681	5.457357	-0.020014	2.443764
99.714298	1915.373721	5.462362	-0.020060	2.448431
100.138753	1923.435063	5.467366	-0.020145	2.453115
100.619391	1931.466212	5.472371	-0.020240	2.457777
100.733459	1939.528276	5.477376	-0.020266	2.462420
101.101940	1947.597727	5.482381	-0.020340	2.467078
101.436651	1955.651885	5.487386	-0.020408	2.471715
101.529026	1963.740385	5.492390	-0.020431	2.476346
101.927835	1971.774937	5.497395	-0.020511	2.480959
102.165597	1979.815167	5.502400	-0.020560	2.485556
102.534147	1987.883169	5.507405	-0.020635	2.490169
102.682270	1995.968479	5.512410	-0.020668	2.494767
102.687054	2004.044852	5.517414	-0.020674	2.499342
103.111470	2012.065007	5.522419	-0.020759	2.503906
103.256639	2020.141050	5.527424	-0.020791	2.508474
103.653133	2028.230641	5.532429	-0.020871	2.513059
103.738861	2036.290987	5.537434	-0.020892	2.517596
103.862969	2044.332617	5.542438	-0.020921	2.522118
104.189723	2052.381214	5.547443	-0.020987	2.526650
104.480215	2060.408318	5.552448	-0.021047	2.531159
104.814655	2068.491341	5.557453	-0.021114	2.535695
105.120515	2076.521471	5.562458	-0.021177	2.540191
105.394387	2084.570098	5.567462	-0.021233	2.544687
105.788531	2092.635298	5.572467	-0.021312	2.549192
105.885779	2100.716055	5.577472	-0.021336	2.553677
106.208225	2108.775488	5.582477	-0.021401	2.558159
106.667913	2116.778142	5.587482	-0.021492	2.562610
106.669525	2124.858546	5.592486	-0.021498	2.567065
106.809802	2132.951403	5.597491	-0.021530	2.571529
107.172925	2140.983424	5.602496	-0.021603	2.575966
107.518724	2149.032275	5.607501	-0.021673	2.580404
107.618319	2157.078745	5.612506	-0.021697	2.584817
107.725837	2165.156051	5.617510	-0.021722	2.589239
107.919385	2173.410576	5.622515	-0.021764	2.593756
108.243697	2181.389619	5.627520	-0.021830	2.598124
108.487383	2189.383734	5.632525	-0.021881	2.602487
108.540471	2197.405669	5.637530	-0.021896	2.606845
108.768815	2205.438009	5.642534	-0.021944	2.611213
109.107785	2213.480602	5.647539	-0.022013	2.615587
109.432870	2221.478424	5.652544	-0.022079	2.619929
109.751900	2229.510458	5.657549	-0.022144	2.624281
109.752569	2237.568678	5.662554	-0.022149	2.628619
110.233637	2245.626862	5.667558	-0.022244	2.632981
110.682715	2253.666832	5.672563	-0.022334	2.637325
110.647053	2261.719592	5.677568	-0.022332	2.641636
111.078204	2269.735167	5.682573	-0.022418	2.645950
111.247909	2277.792348	5.687578	-0.022455	2.650263
111.619318	2285.859464	5.692582	-0.022530	2.654587
111.818928	2293.909000	5.697587	-0.022573	2.658884
111.984823	2301.961682	5.702592	-0.022609	2.663173
112.341166	2310.010725	5.707597	-0.022681	2.667465
112.581035	2318.077683	5.712602	-0.022731	2.671753
112.971463	2326.137688	5.717606	-0.022809	2.676039
113.413304	2334.153123	5.722611	-0.022897	2.680299
113.564478	2342.164001	5.727616	-0.022931	2.684530
113.692592	2350.258692	5.732621	-0.022960	2.688798
114.148298	2358.291106	5.737626	-0.023050	2.693046
114.187203	2366.360489	5.742630	-0.023063	2.697281
114.418720	2374.388390	5.747635	-0.023112	2.701500
114.492342	2382.434203	5.752640	-0.023131	2.705712
114.856045	2390.502709	5.757645	-0.023204	2.709947
114.984994	2398.571996	5.762650	-0.023234	2.714161
115.118295	2406.595753	5.767654	-0.023264	2.718345
115.456827	2414.624907	5.772659	-0.023332	2.722538
115.539909	2422.666359	5.777664	-0.023353	2.726715
115.754891	2430.732860	5.782669	-0.023399	2.730907
116.066652	2438.783484	5.787674	-0.023463	2.735090
116.362461	2446.795875	5.792678	-0.023523	2.739246
116.539026	2454.857750	5.797683	-0.023562	2.743414
116.563306	2462.910540	5.802688	-0.023572	2.747562
116.889506	2471.004941	5.807693	-0.023638	2.751743
117.186294	2479.074529	5.812698	-0.023699	2.755903
117.301923	2487.098536	5.817702	-0.023726	2.760022
117.408892	2495.111810	5.822707	-0.023751	2.764130
117.713352	2503.111487	5.827712	-0.023813	2.768236
117.968503	2511.198184	5.832717	-0.023866	2.772377
118.327024	2519.220049	5.837722	-0.023938	2.776485
118.476367	2527.256282	5.842726	-0.023972	2.780582
118.633323	2535.299270	5.847731	-0.024006	2.784677
119.005304	2543.330440	5.852736	-0.024081	2.788773
119.573933	2551.386602	5.857741	-0.024193	2.792886
119.625105	2559.432108	5.862746	-0.024208	2.796958
119.774841	2567.471792	5.867750	-0.024241	2.801026
120.128086	2575.496672	5.872755	-0.024312	2.805093
119.922043	2583.571784	5.877760	-0.024279	2.809147
120.393982	2591.625833	5.882765	-0.024373	2.813224
120.799579	2599.626021	5.887770	-0.024454	2.817264
120.809006	2607.693313	5.892774	-0.024461	2.821309
121.018771	2615.719311	5.897779	-0.024506	2.825339
121.283876	2623.750572	5.902784	-0.024560	2.829369
121.596977	2631.852431	5.907789	-0.024624	2.833431
121.862590	2639.861817	5.912794	-0.024679	2.837438
122.142401	2647.871651	5.917798	-0.024737	2.841441
122.365670	2655.913186	5.922803	-0.024784	2.845450
122.466093	2663.940454	5.927808	-0.024808	2.849440
122.775468	2672.029160	5.932813	-0.024871	2.853467
122.888780	2680.075221	5.937818	-0.024898	2.857455
122.882760	2688.113172	5.942822	-0.024902	2.861428
123.318686	2696.123345	5.947827	-0.024989	2.865406
123.482541	2704.152627	5.952832	-0.025025	2.869372
124.048286	2712.209639	5.957837	-0.025136	2.873369
124.244285	2720.250276	5.962842	-0.025178	2.877332
124.480114	2728.258836	5.967846	-0.025227	2.881275
124.773803	2736.296910	5.972851	-0.025287	2.885231
125.080018	2744.333940	5.977856	-0.025350	2.889182
125.220586	2752.440818	5.982861	-0.025381	2.893152
125.550696	2760.462368	5.987866	-0.025448	2.897085
125.830743	2768.494782	5.992870	-0.025506	2.901016
125.950048	2776.538689	5.997875	-0.025534	2.904938
126.070812	2784.596592	6.002880	-0.025562	2.908862
126.450813	2792.690307	6.007885	-0.025638	2.912812
126.566650	2800.748228	6.012890	-0.025665	2.916724
126.697242	2808.763799	6.017894	-0.025695	2.920612
127.005798	2816.723464	6.022899	-0.025758	2.924477
127.332667	2824.742940	6.027904	-0.025824	2.928367
127.965093	2832.775536	6.032909	-0.025947	2.932274
128.153890	2840.834453	6.037914	-0.025988	2.936165
128.449288	2848.848401	6.042918	-0.026048	2.940035
128.658285	2856.884406	6.047923	-0.026093	2.943905
128.718904	2864.943933	6.052928	-0.026110	2.947774
129.170073	2872.992704	6.057933	-0.026199	2.951653
129.530686	2881.030747	6.062938	-0.026272	2.955517
129.422640	2889.052874	6.067942	-0.026257	2.959345
129.734458	2897.102355	6.072947	-0.026321	2.963202
129.861327	2905.114839	6.077952	-0.026350	2.967026
129.896222	2913.229652	6.082957	-0.026362	2.970890
130.236571	2921.252692	6.087962	-0.026431	2.974721
130.327690	2929.284588	6.092966	-0.026453	2.978538
130.603005	2937.291386	6.097971	-0.026510	2.982348
130.571210	2945.354460	6.102976	-0.026510	2.986164
130.954311	2953.367243	6.107981	-0.026586	2.989972
131.159863	2961.455586	6.112986	-0.026630	2.993802
131.469918	2969.428752	6.117990	-0.026693	2.997578
131.586347	2977.493614	6.122995	-0.026721	3.001383
131.861499	2985.479659	6.128000	-0.026777	3.005154
131.959687	2993.531748	6.133005	-0.026801	3.008942
132.168973	3001.593688	6.138010	-0.026845	3.012736
132.297600	3009.650370	6.143014	-0.026875	3.016518
132.696956	3017.652190	6.148019	-0.026955	3.020283
133.161779	3025.617277	6.153024	-0.027047	3.024030
133.329768	3033.700391	6.158029	-0.027084	3.027812
133.598698	3041.753725	6.163034	-0.027139	3.031580
133.652592	3049.826156	6.168038	-0.027155	3.035343
133.872673	3057.812828	6.173043	-0.027201	3.039069
134.190476	3065.821496	6.178048	-0.027266	3.042805
134.303001	3073.897744	6.183053	-0.027292	3.046558
134.358200	3081.941396	6.188058	-0.027308	3.050288
134.657064	3089.971875	6.193062	-0.027369	3.054019
135.001878	3098.017753	6.198067	-0.027439	3.057756
135.000403	3106.059778	6.203072	-0.027444	3.061469
135.233194	3114.105209	6.208077	-0.027493	3.065190
135.376775	3122.129645	6.213082	-0.027525	3.068893
135.577716	3130.206896	6.218086	-0.027568	3.072619
135.975960	3138.249509	6.223091	-0.027648	3.076333
136.089230	3146.221409	6.228096	-0.027674	3.079997
136.446832	3154.240115	6.233101	-0.027746	3.083689
136.625021	3162.260846	6.238106	-0.027785	3.087370
136.771518	3170.297863	6.243110	-0.027818	3.091052
136.899795	3178.364849	6.248115	-0.027847	3.094743
136.990875	3186.396662	6.253120	-0.027870	3.098411
137.209756	3194.430701	6.258125	-0.027916	3.102082
137.294668	3202.458286	6.263130	-0.027937	3.105739
137.616371	3210.464143	6.268134	-0.028003	3.109393
137.834397	3218.547731	6.273139	-0.028049	3.113073
137.989932	3226.562502	6.278144	-0.028083	3.116715
138.146936	3234.587967	6.283149	-0.028118	3.120358
138.189592	3242.622507	6.288154	-0.028131	3.123995
138.568859	3250.611674	6.293158	-0.028207	3.127622
139.164691	3258.635278	6.298163	-0.028324	3.131271
139.311490	3266.705915	6.303168	-0.028357	3.134916
139.636683	3274.717826	6.308173	-0.028423	3.138538
139.870752	3282.753675	6.313178	-0.028472	3.142163
139.919634	3290.805963	6.318182	-0.028486	3.145783
140.193313	3298.849736	6.323187	-0.028543	3.149405
140.285187	3306.924155	6.328192	-0.028565	3.153029
140.611314	3314.946012	6.333197	-0.028632	3.156634
140.678342	3322.959809	6.338202	-0.028650	3.160221
140.869422	3330.942737	6.343206	-0.028691	3.163796
141.281069	3338.988334	6.348211	-0.028773	3.167403
141.447054	3347.015206	6.353216	-0.028809	3.170988
141.477964	3355.086040	6.358221	-0.028820	3.174582
141.840000	3363.076550	6.363226	-0.028893	3.178151
141.921611	3371.134126	6.368230	-0.028914	3.181734
142.052016	3379.169397	6.373235	-0.028944	3.185304
141.982363	3387.206827	6.378240	-0.028936	3.188863
142.497989	3395.245283	6.383245	-0.029038	3.192444
142.818466	3403.283375	6.388250	-0.029103	3.196012
142.936723	3411.271349	6.393254	-0.029130	3.199545
143.298014	3419.295415	6.398259	-0.029203	3.203100
143.495121	3427.311534	6.403264	-0.029245	3.206641
143.663586	3435.393256	6.408269	-0.029282	3.210206
143.682008	3443.439247	6.413274	-0.029291	3.213745
143.811577	3451.470145	6.418278	-0.029321	3.217277
144.287387	3459.480967	6.423283	-0.029415	3.220812
144.194224	3467.495026	6.428288	-0.029403	3.224320
144.626747	3475.519244	6.433293	-0.029489	3.227851
144.595622	3483.607908	6.438298	-0.029489	3.231387
144.841760	3491.653844	6.443302	-0.029540	3.234912
145.364468	3499.637865	6.448307	-0.029643	3.238417
145.375564	3507.635993	6.453312	-0.029650	3.241903
145.440221	3515.675809	6.458317	-0.029668	3.245407
145.733128	3523.652983	6.463322	-0.029728	3.248888
146.076519	3531.716174	6.468326	-0.029797	3.252405
146.281034	3539.824080	6.473331	-0.029841	3.255932
146.388308	3547.772560	6.478336	-0.029866	3.259382
146.648609	3555.809992	6.483341	-0.029920	3.262873
146.597060	3563.884680	6.488346	-0.029916	3.266364
146.742625	3571.892175	6.493350	-0.029949	3.269830
147.260812	3579.955367	6.498355	-0.030051	3.273331
147.270288	3587.982392	6.503360	-0.030058	3.276793
147.477821	3595.991261	6.508365	-0.030102	3.280251
147.668381	3603.984090	6.513370	-0.030143	3.283697
147.839277	3612.022801	6.518374	-0.030181	3.287159
148.100199	3620.073608	6.523379	-0.030235	3.290626
148.321198	3628.116236	6.528384	-0.030281	3.294085
148.662837	3636.118704	6.533389	-0.030350	3.297527
149.054472	3644.133258	6.538394	-0.030429	3.300972
148.981719	3652.165705	6.543398	-0.030421	3.304404
149.452054	3660.199041	6.548403	-0.030514	3.307853
149.680889	3668.229522	6.553408	-0.030562	3.311288
149.983195	3676.313243	6.558413	-0.030624	3.314745
150.127307	3684.305848	6.563418	-0.030656	3.318154
150.360354	3692.319456	6.568422	-0.030705	3.321571
150.617773	3700.315764	6.573427	-0.030758	3.324978
150.708001	3708.347616	6.578432	-0.030781	3.328391
150.672724	3716.425293	6.583437	-0.030780	3.331815
150.802983	3724.490880	6.588442	-0.030809	3.335236
150.924366	3732.468895	6.593446	-0.030837	3.338617
151.282994	3740.509016	6.598451	-0.030910	3.342029
151.541459	3748.487097	6.603456	-0.030963	3.345408
151.499166	3756.559443	6.608461	-0.030961	3.348811
151.581685	3764.619549	6.613466	-0.030982	3.352211
151.807153	3772.646604	6.618470	-0.031029	3.355599
152.121936	3780.649679	6.623475	-0.031093	3.358976
152.212058	3788.659468	6.628480	-0.031116	3.362345
152.331331	3796.720234	6.633485	-0.031143	3.365733
152.845470	3804.704733	6.638490	-0.031244	3.369099
153.064002	3812.767455	6.643494	-0.031291	3.372484
153.037047	3820.843630	6.648499	-0.031291	3.375863
153.442310	3828.800740	6.653504	-0.031372	3.379204
153.835464	3836.841744	6.658509	-0.031451	3.382576
153.743006	3844.882644	6.663514	-0.031439	3.385927
153.877960	3852.913025	6.668518	-0.031470	3.389279
153.970311	3861.042036	6.673523	-0.031492	3.392667
153.987809	3869.041336	6.678528	-0.031501	3.395995
154.437139	3876.994256	6.683533	-0.031590	3.399316
154.641475	3885.007264	6.688538	-0.031634	3.402649
154.614321	3893.043032	6.693542	-0.031634	3.405981
155.037515	3901.037862	6.698547	-0.031718	3.409308
155.285532	3909.067332	6.703552	-0.031770	3.412641
155.504732	3917.126048	6.708557	-0.031816	3.415980
155.577909	3925.123172	6.713562	-0.031836	3.419287
155.707621	3933.124173	6.718566	-0.031865	3.422593
156.024357	3941.172137	6.723571	-0.031930	3.425922
156.200288	3949.197935	6.728576	-0.031968	3.429234
156.320453	3957.269548	6.733581	-0.031996	3.432560
156.663847	3965.305742	6.738586	-0.032065	3.435875
157.016458	3973.253289	6.743590	-0.032136	3.439151
157.213153	3981.293582	6.748595	-0.032178	3.442456
157.101531	3989.323276	6.753600	-0.032163	3.445744
157.572953	3997.337825	6.758605	-0.032256	3.449042
157.401538	4005.433540	6.763610	-0.032230	3.452348
157.781567	4013.414590	6.768614	-0.032306	3.455623
158.190457	4021.450797	6.773619	-0.032388	3.458918
158.148033	4029.470544	6.778624	-0.032385	3.462188
158.519194	4037.507717	6.783629	-0.032460	3.465476
158.866141	4045.527786	6.788634	-0.032530	3.468753
159.048813	4053.596318	6.793638	-0.032570	3.472041
159.238262	4061.625939	6.798643	-0.032610	3.475310
159.490677	4069.637461	6.803648	-0.032663	3.478571
159.792457	4077.635786	6.808653	-0.032725	3.481825
159.761678	4085.651751	6.813658	-0.032724	3.485073
159.926386	4093.676798	6.818662	-0.032760	3.488327
160.272772	4101.711399	6.823667	-0.032830	3.491588
160.357250	4109.739376	6.828672	-0.032852	3.494835
160.522187	4117.774005	6.833677	-0.032888	3.498084
160.686228	4125.783734	6.838682	-0.032924	3.501320
160.964226	4133.768860	6.843686	-0.032981	3.504547
161.326932	4141.807679	6.848691	-0.033054	3.507794
161.344346	4149.868360	6.853696	-0.033063	3.511037
161.550186	4157.911892	6.858701	-0.033107	3.514276
161.749445	4165.912106	6.863706	-0.033149	3.517494
161.859777	4173.937462	6.868710	-0.033175	3.520717
162.086457	4181.932499	6.873715	-0.033223	3.523928
162.212450	4189.955877	6.878720	-0.033252	3.527144
162.444469	4198.016061	6.883725	-0.033301	3.530375
162.727175	4206.044730	6.888730	-0.033359	3.533593
162.976871	4214.077093	6.893734	-0.033411	3.536807
163.134703	4222.127733	6.898739	-0.033446	3.540024
163.445300	4230.091988	6.903744	-0.033509	3.543207
163.566792	4238.177371	6.908749	-0.033537	3.546430
163.470934	4246.216572	6.913754	-0.033525	3.549626
163.800040	4254.300397	6.918758	-0.033591	3.552848
164.423650	4262.344617	6.923763	-0.033713	3.556061
164.344239	4270.288028	6.928768	-0.033704	3.559210
164.483114	4278.309735	6.933773	-0.033735	3.562394
164.709902	4286.307744	6.938778	-0.033783	3.565568
164.979103	4294.268816	6.943782	-0.033838	3.568726
165.248963	4302.367386	6.948787	-0.033894	3.571936
165.259228	4310.378528	6.953792	-0.033902	3.575100
165.612679	4318.378016	6.958797	-0.033973	3.578267
165.800839	4326.431672	6.963802	-0.034013	3.581448
165.742840	4334.421678	6.968806	-0.034008	3.584594
165.929558	4342.490611	6.973811	-0.034048	3.587775
166.197566	4350.489427	6.978816	-0.034104	3.590927
166.538460	4358.521150	6.983821	-0.034173	3.594093
166.582935	4366.537678	6.988826	-0.034186	3.597240
166.896274	4374.537980	6.993830	-0.034250	3.600387
166.935686	4382.578585	6.998835	-0.034263	3.603539
166.841117	4390.608690	7.003840	-0.034251	3.606680
167.197071	4398.608104	7.008845	-0.034323	3.609818
167.549537	4406.657256	7.013850	-0.034394	3.612974
167.583975	4414.704126	7.018854	-0.034406	3.616117
167.932556	4422.691810	7.023859	-0.034476	3.619242
168.144377	4430.699396	7.028864	-0.034521	3.622369
168.185169	4438.738844	7.033869	-0.034534	3.625501
168.211469	4446.816788	7.038874	-0.034544	3.628645
168.667973	4454.812270	7.043878	-0.034635	3.631766
168.843969	4462.879401	7.048883	-0.034673	3.634904
168.857035	4470.865105	7.053888	-0.034681	3.638004
169.376732	4478.893444	7.058893	-0.034783	3.641131
169.399009	4486.881838	7.063898	-0.034793	3.644226
169.481695	4494.909192	7.068902	-0.034814	3.647336
169.789604	4502.960285	7.073907	-0.034877	3.650458
169.730289	4510.996673	7.078912	-0.034871	3.653562
169.784991	4519.032902	7.083917	-0.034887	3.656666
170.067899	4527.052364	7.088922	-0.034945	3.659767
170.125590	4535.008961	7.093926	-0.034961	3.662835
170.489426	4543.091852	7.098931	-0.035034	3.665958
170.692998	4551.079790	7.103936	-0.035078	3.669037
170.982656	4559.128050	7.108941	-0.035137	3.672138
171.338924	4567.164961	7.113946	-0.035209	3.675235
171.220752	4575.160801	7.118950	-0.035193	3.678300
171.570398	4583.211068	7.123955	-0.035263	3.681397
171.756991	4591.177224	7.128960	-0.035303	3.684454
171.894317	4599.218621	7.133965	-0.035334	3.687536
171.940391	4607.253250	7.138970	-0.035348	3.690610
172.200902	4615.268214	7.143974	-0.035402	3.693680
172.497111	4623.316250	7.148979	-0.035463	3.696761
172.554561	4631.308201	7.153984	-0.035479	3.699812
172.794598	4639.345645	7.158989	-0.035529	3.702882
172.923333	4647.386466	7.163994	-0.035559	3.705948
172.876600	4655.372372	7.168998	-0.035556	3.708986
173.331056	4663.458839	7.174003	-0.035646	3.712073
173.608427	4671.499564	7.179008	-0.035703	3.715135
173.977026	4679.475369	7.184013	-0.035777	3.718172
174.018115	4687.482172	7.189018	-0.035790	3.721210
174.355429	4695.413970	7.194022	-0.035858	3.724225
174.565862	4703.518784	7.199027	-0.035903	3.727299
174.627424	4711.518526	7.204032	-0.035920	3.730328
174.950084	4719.550382	7.209037	-0.035986	3.733373
175.097824	4727.599172	7.214042	-0.036019	3.736417
175.193615	4735.594989	7.219046	-0.036042	3.739437
175.457333	4743.640599	7.224051	-0.036097	3.742478
175.697733	4751.637981	7.229056	-0.036147	3.745498
175.825922	4759.688746	7.234061	-0.036176	3.748532
175.844858	4767.741276	7.239066	-0.036185	3.751563
176.319410	4775.707272	7.244070	-0.036279	3.754569
176.420891	4783.780259	7.249075	-0.036303	3.757603
176.290997	4791.790873	7.254080	-0.036285	3.760607
176.689373	4799.792042	7.259085	-0.036364	3.763617
176.805634	4807.856249	7.264090	-0.036392	3.766642
177.034678	4815.823351	7.269094	-0.036440	3.769630
177.476769	4823.913314	7.274099	-0.036527	3.772667
177.510625	4831.891057	7.279104	-0.036539	3.775650
177.712491	4839.905944	7.284109	-0.036582	3.778648
177.873988	4847.976588	7.289114	-0.036618	3.781664
178.139691	4855.922707	7.294118	-0.036673	3.784633
178.452508	4864.019883	7.299123	-0.036737	3.787658
178.471359	4872.017914	7.304128	-0.036746	3.790636
178.674991	4880.101084	7.309133	-0.036789	3.793648
178.974543	4888.099390	7.314138	-0.036850	3.796628
179.008048	4896.050054	7.319142	-0.036862	3.799582
179.160711	4904.088263	7.324147	-0.036896	3.802569
179.420357	4912.073529	7.329152	-0.036950	3.805536
179.562564	4920.112476	7.334157	-0.036982	3.808518
179.570987	4928.133544	7.339162	-0.036989	3.811488
179.876256	4936.152910	7.344166	-0.037051	3.814462
180.256921	4944.169238	7.349171	-0.037127	3.817434
180.236360	4952.173725	7.354176	-0.037129	3.820390
180.259107	4960.245378	7.359181	-0.037139	3.823370
180.593701	4968.247033	7.364186	-0.037207	3.826329
180.675501	4976.280499	7.369190	-0.037227	3.829291
180.941465	4984.313132	7.374195	-0.037282	3.832255
181.173477	4992.308201	7.379200	-0.037331	3.835202
181.188272	5000.304827	7.384205	-0.037339	3.838142
181.736689	5008.338721	7.389210	-0.037447	3.841105
181.785241	5016.290596	7.394214	-0.037461	3.844026
182.148449	5024.373112	7.399219	-0.037534	3.846998
182.021241	5032.387159	7.404224	-0.037516	3.849933
182.020561	5040.456518	7.409229	-0.037522	3.852889
182.246612	5048.515253	7.414234	-0.037569	3.855843
182.418711	5056.494435	7.419238	-0.037607	3.858764
182.644694	5064.539172	7.424243	-0.037654	3.861709
182.751884	5072.496593	7.429248	-0.037680	3.864617
183.272154	5080.552197	7.434253	-0.037782	3.867566
183.411246	5088.601522	7.439258	-0.037813	3.870504
183.288930	5096.827233	7.444262	-0.037796	3.873498
183.635998	5104.839146	7.449267	-0.037866	3.876422
183.793201	5112.740415	7.454272	-0.037901	3.879299
183.974509	5120.727099	7.459277	-0.037940	3.882205
184.039646	5128.704566	7.464282	-0.037958	3.885104
184.216871	5136.697546	7.469286	-0.037996	3.888009
184.389717	5144.755379	7.474291	-0.038034	3.890934
184.660486	5152.762472	7.479296	-0.038090	3.893841
184.855367	5160.804681	7.484301	-0.038132	3.896757
184.923297	5168.788892	7.489306	-0.038150	3.899647
184.932037	5176.786477	7.494310	-0.038157	3.902539
185.176575	5184.799332	7.499315	-0.038208	3.905439
185.251622	5192.846083	7.504320	-0.038227	3.908346
185.533679	5200.891623	7.509325	-0.038285	3.911253
185.733217	5208.886885	7.514330	-0.038328	3.914139
186.030574	5216.936009	7.519334	-0.038389	3.917044
186.191366	5224.912326	7.524339	-0.038424	3.919919
186.191654	5232.929665	7.529344	-0.038430	3.922802
186.445926	5240.938288	7.534349	-0.038483	3.925685
186.572800	5248.968049	7.539354	-0.038512	3.928572
186.586814	5256.985963	7.544358	-0.038520	3.931450
186.971273	5265.040827	7.549363	-0.038597	3.934345
187.170810	5273.043930	7.554368	-0.038640	3.937217
187.134970	5281.057702	7.559373	-0.038638	3.940086
187.489861	5289.087617	7.564378	-0.038710	3.942966
187.681435	5297.082712	7.569382	-0.038751	3.945828
187.536547	5305.151816	7.574387	-0.038730	3.948709
187.628340	5313.140817	7.579392	-0.038752	3.951563
187.751253	5321.209401	7.584397	-0.038781	3.954444
188.058197	5329.188266	7.589402	-0.038843	3.957294
188.094948	5337.169441	7.594406	-0.038855	3.960138
188.419605	5345.225838	7.599411	-0.038921	3.963012
188.488619	5353.240805	7.604416	-0.038940	3.965864
188.679706	5361.229387	7.609421	-0.038981	3.968708
189.013996	5369.261804	7.614426	-0.039048	3.971567
189.234357	5377.280928	7.619430	-0.039095	3.974417
189.465941	5385.334434	7.624435	-0.039144	3.977278
189.463394	5393.315868	7.629440	-0.039149	3.980107
189.964694	5401.327000	7.634445	-0.039247	3.982953
190.044254	5409.383165	7.639450	-0.039268	3.985806
190.050610	5417.377022	7.644454	-0.039274	3.988634
190.376279	5425.481081	7.649459	-0.039341	3.991503
190.327474	5433.486338	7.654464	-0.039337	3.994330
190.417862	5441.517417	7.659469	-0.039359	3.997166
190.676612	5449.481914	7.664474	-0.039413	3.999979
190.908327	5457.509190	7.669478	-0.039462	4.002812
190.887121	5465.529768	7.674483	-0.039463	4.005637
191.201721	5473.517794	7.679488	-0.039527	4.008453
191.339621	5481.604760	7.684493	-0.039558	4.011299
191.539691	5489.635218	7.689498	-0.039601	4.014125
191.571533	5497.671798	7.694502	-0.039612	4.016948
191.751416	5505.661218	7.699507	-0.039651	4.019754
192.127604	5513.646756	7.704512	-0.039727	4.022561
192.058360	5521.687006	7.709517	-0.039720	4.025377
192.398135	5529.735494	7.714522	-0.039788	4.028201
192.503851	5537.743746	7.719526	-0.039813	4.031005
192.759235	5545.835088	7.724531	-0.039867	4.033839
192.836655	5553.817478	7.729536	-0.039886	4.036630
193.161797	5561.765282	7.734541	-0.039952	4.039410
193.285903	5569.796208	7.739546	-0.039981	4.042215
193.345696	5577.777298	7.744550	-0.039998	4.044999
193.649342	5585.826179	7.749555	-0.040060	4.047808
193.838646	5593.833595	7.754560	-0.040100	4.050600
193.966486	5601.886892	7.759565	-0.040130	4.053404
194.126791	5609.931002	7.764570	-0.040165	4.056204
194.360502	5617.863562	7.769574	-0.040214	4.058964
194.657926	5625.931184	7.774579	-0.040275	4.061770
194.776106	5633.885013	7.779584	-0.040302	4.064532
195.052503	5641.972002	7.784589	-0.040359	4.067341
195.185725	5649.995750	7.789594	-0.040390	4.070123
195.359328	5658.001770	7.794598	-0.040427	4.072899
195.620891	5666.030531	7.799603	-0.040482	4.075681
195.654967	5674.005415	7.804608	-0.040493	4.078439
195.732214	5682.014716	7.809613	-0.040513	4.081209
195.960962	5690.028888	7.814618	-0.040561	4.083980
195.947014	5698.045557	7.819622	-0.040564	4.086747
196.280406	5706.061205	7.824627	-0.040632	4.089516
196.193811	5714.148752	7.829632	-0.040621	4.092302
196.483465	5722.141858	7.834637	-0.040681	4.095059
196.971142	5730.134600	7.839642	-0.040777	4.097817
196.967136	5738.154669	7.844646	-0.040782	4.100575
197.066318	5746.199798	7.849651	-0.040806	4.103342
197.450310	5754.212231	7.854656	-0.040882	4.106099
197.572618	5762.229263	7.859661	-0.040911	4.108853
197.875950	5770.293127	7.864666	-0.040973	4.111623
197.951779	5778.318297	7.869670	-0.040992	4.114375
198.204465	5786.345895	7.874675	-0.041045	4.117129
198.105621	5794.299040	7.879680	-0.041032	4.119850
198.402461	5802.331277	7.884685	-0.041093	4.122602
198.829634	5810.387040	7.889690	-0.041178	4.125361
198.887922	5818.371428	7.894694	-0.041194	4.128090
199.155373	5826.387336	7.899699	-0.041249	4.130830
199.119669	5834.437088	7.904704	-0.041248	4.133576
199.168467	5842.505620	7.909709	-0.041263	4.136328
199.002530	5850.488283	7.914714	-0.041237	4.139046
199.394472	5858.497466	7.919718	-0.041316	4.141778
199.479037	5866.512020	7.924723	-0.041337	4.144506
199.490946	5874.536302	7.929728	-0.041345	4.147235
199.793450	5882.544639	7.934733	-0.041406	4.149961
200.223650	5890.596210	7.939738	-0.041492	4.152700
200.162031	5898.647376	7.944742	-0.041486	4.155432
200.257092	5906.642237	7.949747	-0.041509	4.158145
200.443341	5914.631861	7.954752	-0.041549	4.160855
200.749836	5922.630044	7.959757	-0.041612	4.163567
200.925020	5930.697087	7.964762	-0.041650	4.166300
201.004980	5938.635164	7.969766	-0.041670	4.168986
201.047614	5946.743173	7.974771	-0.041684	4.171728
201.107557	5954.733937	7.979776	-0.041701	4.174428
201.183220	5962.746961	7.984781	-0.041720	4.177134
201.530319	5970.738672	7.989786	-0.041790	4.179834
201.658690	5978.722502	7.994790	-0.041820	4.182528
202.023253	5986.754809	7.999795	-0.041893	4.185238
201.956245	5994.825954	8.004800	-0.041886	4.187955
202.086847	6002.816138	8.009805	-0.041916	4.190646
202.268930	6010.955668	8.014810	-0.041955	4.193385
202.333324	6018.954739	8.019814	-0.041973	4.196074
202.670868	6026.847115	8.024819	-0.042041	4.198728
202.875484	6034.888381	8.029824	-0.042085	4.201429
202.804746	6042.842967	8.034829	-0.042077	4.204097
203.344557	6050.910320	8.039834	-0.042183	4.206807
203.288786	6058.892417	8.044838	-0.042178	4.209480
203.415424	6066.959800	8.049843	-0.042207	4.212182
203.350968	6074.975707	8.054848	-0.042200	4.214863
203.682399	6082.960423	8.059853	-0.042268	4.217536
203.564001	6090.961082	8.064858	-0.042251	4.220208
203.712850	6098.992449	8.069862	-0.042284	4.222892
204.025215	6106.997932	8.074867	-0.042348	4.225566
204.324208	6115.036174	8.079872	-0.042409	4.228250
204.360021	6123.042390	8.084877	-0.042421	4.230919
204.513762	6131.128074	8.089882	-0.042455	4.233613
204.536320	6139.141148	8.094886	-0.042465	4.236281
204.579625	6147.132407	8.099891	-0.042479	4.238939
204.892560	6155.132286	8.104896	-0.042542	4.241602
205.119600	6163.091820	8.109901	-0.042590	4.244248
205.307784	6171.164746	8.114906	-0.042631	4.246931
205.561930	6179.127130	8.119910	-0.042683	4.249575
205.955620	6187.243284	8.124915	-0.042762	4.252270
205.974281	6195.269543	8.129920	-0.042771	4.254930
205.788844	6203.262105	8.134925	-0.042742	4.257575
206.058199	6211.280237	8.139930	-0.042798	4.260231
206.297727	6219.272193	8.144934	-0.042848	4.262877
206.281811	6227.327078	8.149939	-0.042850	4.265539
206.407783	6235.330285	8.154944	-0.042879	4.268184
206.765654	6243.365502	8.159949	-0.042951	4.270840
206.996008	6251.433827	8.164954	-0.043000	4.273504
207.011088	6259.450374	8.169958	-0.043008	4.276147
207.219874	6267.408137	8.174963	-0.043052	4.278772
207.333436	6275.453923	8.179968	-0.043079	4.281422
207.460099	6283.386751	8.184973	-0.043108	4.284034
207.788573	6291.482702	8.189978	-0.043175	4.286700
207.869514	6299.424713	8.194982	-0.043195	4.289311
208.228797	6307.535813	8.199987	-0.043268	4.291978
208.259721	6315.524173	8.204992	-0.043279	4.294601
208.410073	6323.560206	8.209997	-0.043312	4.297239
208.571130	6331.546696	8.215002	-0.043348	4.299859
208.536090	6339.571439	8.220006	-0.043347	4.302488
208.738258	6347.601146	8.225011	-0.043390	4.305119
208.986384	6355.584194	8.230016	-0.043442	4.307734
209.049373	6363.632880	8.235021	-0.043459	4.310367
209.151975	6371.703750	8.240026	-0.043483	4.313006
209.320457	6379.671981	8.245030	-0.043520	4.315611
209.424899	6387.688654	8.250035	-0.043545	4.318229
209.408385	6395.682361	8.255040	-0.043548	4.320837
209.527805	6403.663474	8.260045	-0.043575	4.323440
210.062725	6411.713972	8.265050	-0.043680	4.326068
210.150876	6419.714265	8.270054	-0.043702	4.328674
210.332394	6427.805647	8.275059	-0.043742	4.331309
210.578444	6435.797911	8.280064	-0.043793	4.333910
210.487116	6443.804268	8.285069	-0.043781	4.336513
210.668444	6451.807667	8.290074	-0.043821	4.339114
210.908374	6459.819519	8.295078	-0.043871	4.341717
211.166266	6467.804150	8.300083	-0.043924	4.344310
211.199212	6475.873441	8.305088	-0.043936	4.346927
211.366754	6483.848496	8.310093	-0.043972	4.349513
211.355417	6491.927461	8.315098	-0.043976	4.352130
211.353387	6499.982164	8.320102	-0.043981	4.354738
211.656490	6507.998928	8.325107	-0.044043	4.357333
211.799757	6515.948427	8.330112	-0.044075	4.359905
211.827934	6523.958091	8.335117	-0.044086	4.362493
212.060864	6531.933748	8.340122	-0.044135	4.365070
212.296413	6539.962550	8.345126	-0.044184	4.367663
212.369041	6547.974148	8.350131	-0.044203	4.370248
212.541762	6555.996393	8.355136	-0.044241	4.372835
212.568892	6564.035870	8.360141	-0.044251	4.375425
213.018635	6572.057799	8.365146	-0.044340	4.378011
213.120874	6580.037615	8.370150	-0.044365	4.380579
213.495774	6588.058031	8.375155	-0.044440	4.383161
213.630903	6596.079837	8.380160	-0.044471	4.385740
213.673922	6604.100273	8.385165	-0.044484	4.388317
213.791200	6612.139718	8.390170	-0.044512	4.390898
213.907636	6620.180070	8.395174	-0.044539	4.393479
214.097277	6628.211295	8.400179	-0.044580	4.396055
214.174165	6636.158587	8.405184	-0.044599	4.398602
214.341102	6644.179228	8.410189	-0.044636	4.401172
214.567777	6652.160719	8.415194	-0.044684	4.403728
214.605851	6660.209565	8.420198	-0.044696	4.406303
214.800120	6668.265515	8.425203	-0.044738	4.408879
214.922892	6676.292213	8.430208	-0.044766	4.411445
215.288245	6684.285607	8.435213	-0.044840	4.413999
215.292398	6692.340265	8.440218	-0.044846	4.416570
215.248563	6700.287765	8.445222	-0.044843	4.419105
215.768100	6708.406666	8.450227	-0.044946	4.421695
215.529609	6716.362464	8.455232	-0.044907	4.424229
215.791625	6724.396776	8.460237	-0.044961	4.426788
216.228857	6732.393070	8.465242	-0.045048	4.429335
216.063570	6740.451876	8.470246	-0.045022	4.431897
216.361638	6748.485161	8.475251	-0.045083	4.434452
216.428506	6756.495952	8.480256	-0.045101	4.436997
216.452391	6764.466720	8.485261	-0.045111	4.439528
216.469245	6772.522854	8.490266	-0.045120	4.442084
216.608550	6780.444139	8.495270	-0.045151	4.444596
216.816325	6788.571063	8.500275	-0.045196	4.447173
217.054964	6796.510138	8.505280	-0.045245	4.449689
217.149040	6804.569100	8.510285	-0.045268	4.452240
217.316517	6812.615027	8.515290	-0.045305	4.454787
217.267079	6820.636714	8.520294	-0.045301	4.457323
217.381849	6828.606608	8.525299	-0.045328	4.459842
217.442413	6836.637081	8.530304	-0.045345	4.462379
217.638048	6844.617139	8.535309	-0.045387	4.464898
217.680501	6852.679789	8.540314	-0.045400	4.467442
217.682902	6860.643520	8.545318	-0.045406	4.469953
218.117309	6868.705993	8.550323	-0.045493	4.472496
217.997461	6876.731746	8.555328	-0.045476	4.475023
218.084654	6884.743882	8.560333	-0.045497	4.477545
218.299930	6892.718516	8.565338	-0.045543	4.480055
218.625232	6900.710471	8.570343	-0.045609	4.482568
218.763728	6908.750703	8.575347	-0.045640	4.485095
219.187739	6916.766810	8.580352	-0.045725	4.487614
219.576607	6924.815802	8.585357	-0.045803	4.490142
219.533279	6932.850767	8.590362	-0.045800	4.492662
219.636686	6940.826095	8.595367	-0.045825	4.495163
220.112619	6948.873222	8.600371	-0.045919	4.497686
220.212954	6956.865646	8.605376	-0.045943	4.500189
220.238939	6964.880190	8.610381	-0.045953	4.502698
220.553003	6972.886738	8.615386	-0.046017	4.505203
220.427041	6980.937569	8.620391	-0.045999	4.507720
220.569668	6988.957649	8.625395	-0.046031	4.510226
220.770955	6997.014779	8.630400	-0.046074	4.512743
220.973270	7004.987437	8.635405	-0.046117	4.515231
221.177484	7013.016625	8.640410	-0.046161	4.517737
221.229732	7020.960346	8.645415	-0.046176	4.520213
221.493255	7028.998110	8.650419	-0.046231	4.522718
221.623535	7036.990249	8.655424	-0.046260	4.525207
221.728635	7045.006085	8.660429	-0.046285	4.527703
221.891671	7053.026003	8.665434	-0.046321	4.530198
222.124425	7061.067034	8.670439	-0.046370	4.532698
222.211865	7069.083377	8.675443	-0.046392	4.535189
222.239582	7077.082414	8.680448	-0.046403	4.537673
222.622326	7085.084745	8.685453	-0.046479	4.540158
222.771284	7093.137260	8.690458	-0.046513	4.542656
222.691823	7101.098849	8.695463	-0.046503	4.545124
223.183871	7109.167492	8.700467	-0.046600	4.547625
223.084653	7117.182329	8.705472	-0.046587	4.550107
223.406729	7125.212530	8.710477	-0.046653	4.552593
223.348140	7133.266237	8.715482	-0.046647	4.555085
223.348622	7141.217005	8.720487	-0.046653	4.557543
223.720865	7149.233094	8.725491	-0.046728	4.560021
223.948005	7157.261384	8.730496	-0.046775	4.562500
223.948448	7165.223219	8.735501	-0.046781	4.564958
224.011828	7173.287299	8.740506	-0.046798	4.567446
223.946706	7181.276265	8.745511	-0.046792	4.569909
224.250267	7189.364527	8.750515	-0.046854	4.572402
224.467539	7197.360276	8.755520	-0.046900	4.574865
224.650619	7205.379805	8.760525	-0.046939	4.577334
224.840811	7213.358049	8.765530	-0.046980	4.579789
225.138068	7221.375916	8.770535	-0.047041	4.582255
225.313267	7229.386333	8.775539	-0.047079	4.584717
225.242135	7237.415920	8.780544	-0.047071	4.587183
225.281489	7245.450600	8.785549	-0.047084	4.589650
225.749614	7253.542767	8.790554	-0.047177	4.592133
225.623759	7261.518300	8.795559	-0.047159	4.594579
225.853540	7269.578007	8.800563	-0.047207	4.597049
225.919682	7277.489446	8.805568	-0.047225	4.599473
225.931042	7285.535704	8.810573	-0.047232	4.601936
225.983612	7293.537266	8.815578	-0.047248	4.604385
226.106835	7301.547151	8.820583	-0.047276	4.606835
226.458127	7309.561241	8.825587	-0.047347	4.609285
226.663682	7317.618626	8.830592	-0.047391	4.611746
226.821326	7325.592459	8.835597	-0.047426	4.614181
226.984677	7333.671874	8.840602	-0.047461	4.616647
226.979020	7341.639946	8.845607	-0.047466	4.619077
227.187025	7349.678902	8.850611	-0.047510	4.621528
227.318537	7357.618652	8.855616	-0.047540	4.623947
227.371313	7365.695856	8.860621	-0.047555	4.626407
227.555271	7373.703655	8.865626	-0.047595	4.628845
227.819206	7381.691219	8.870631	-0.047650	4.631274
227.923470	7389.788645	8.875635	-0.047675	4.633736
227.902228	7397.808013	8.880640	-0.047676	4.636173
228.020100	7405.752687	8.885645	-0.047704	4.638586
228.505539	7413.808252	8.890650	-0.047799	4.641032
228.549524	7421.732452	8.895655	-0.047813	4.643436
228.420909	7429.823071	8.900659	-0.047795	4.645889
228.597784	7437.796114	8.905664	-0.047833	4.648306
228.796579	7445.846636	8.910669	-0.047876	4.650744
228.951827	7453.861113	8.915674	-0.047910	4.653171
229.095395	7461.889093	8.920679	-0.047942	4.655600
229.315402	7469.889581	8.925683	-0.047989	4.658020
229.559421	7477.893375	8.930688	-0.048039	4.660439
229.611379	7485.897604	8.935693	-0.048055	4.662857
229.925605	7493.940152	8.940698	-0.048119	4.665285
229.857651	7501.952317	8.945703	-0.048111	4.667704
229.827972	7509.957399	8.950707	-0.048111	4.670119
230.134742	7518.041693	8.955712	-0.048174	4.672556
230.161106	7526.067861	8.960717	-0.048184	4.674974
230.238184	7534.050761	8.965722	-0.048204	4.677379
230.356651	7541.967478	8.970727	-0.048232	4.679762
230.657528	7550.081269	8.975731	-0.048293	4.682202
230.760117	7557.968825	8.980736	-0.048318	4.684574
230.982326	7566.051244	8.985741	-0.048365	4.687003
231.169017	7574.056656	8.990746	-0.048405	4.689408
231.144607	7582.098250	8.995751	-0.048406	4.691822
231.378557	7590.119599	9.000755	-0.048455	4.694229
231.546097	7598.162432	9.005760	-0.048492	4.696641
231.472619	7606.128691	9.010765	-0.048483	4.699029
231.729663	7614.183595	9.015770	-0.048537	4.701442
231.974310	7622.127954	9.020775	-0.048588	4.703821
232.143141	7630.213599	9.025779	-0.048625	4.706241
232.313521	7638.201195	9.030784	-0.048662	4.708630
232.188235	7646.193788	9.035789	-0.048644	4.711020
232.330478	7654.301172	9.040794	-0.048676	4.713443
232.351344	7662.273817	9.045799	-0.048685	4.715824
232.450447	7670.243831	9.050803	-0.048709	4.718204
232.702769	7678.263162	9.055808	-0.048762	4.720596
232.687211	7686.238283	9.060813	-0.048764	4.722975
232.883244	7694.329289	9.065818	-0.048806	4.725386
232.864670	7702.357592	9.070823	-0.048808	4.727778
233.111692	7710.356760	9.075827	-0.048860	4.730160
233.247344	7718.393636	9.080832	-0.048891	4.732552
233.344241	7726.417470	9.085837	-0.048914	4.734938
233.710844	7734.413387	9.090842	-0.048988	4.737315
233.583007	7742.393809	9.095847	-0.048970	4.739687
233.799631	7750.455293	9.100851	-0.049015	4.742081
234.045481	7758.422375	9.105856	-0.049067	4.744445
234.010556	7766.444231	9.110861	-0.049066	4.746826
234.323990	7774.495976	9.115866	-0.049129	4.749213
234.259873	7782.504565	9.120871	-0.049123	4.751587
234.643664	7790.582225	9.125875	-0.049200	4.753979
234.671141	7798.567262	9.130880	-0.049211	4.756344
234.748774	7806.526277	9.135885	-0.049230	4.758700
234.905497	7814.560924	9.140890	-0.049265	4.761076
234.943279	7822.535924	9.145895	-0.049278	4.763434
235.046636	7830.570638	9.150899	-0.049302	4.765808
235.247100	7838.548235	9.155904	-0.049345	4.768164
235.454541	7846.606101	9.160909	-0.049389	4.770543
235.365246	7854.660066	9.165914	-0.049378	4.772920
235.529170	7862.703296	9.170919	-0.049414	4.775291
235.815683	7870.654752	9.175923	-0.049473	4.777635
235.972432	7878.651953	9.180928	-0.049508	4.779990
236.025790	7886.652831	9.185933	-0.049523	4.782347
236.356359	7894.659360	9.190938	-0.049590	4.784702
236.468903	7902.718946	9.195943	-0.049616	4.787073
236.429738	7910.686995	9.200947	-0.049615	4.789416
236.634293	7918.805849	9.205952	-0.049658	4.791802
236.572099	7926.759151	9.210957	-0.049652	4.794139
236.733358	7934.845088	9.215962	-0.049688	4.796512
236.833991	7942.722464	9.220967	-0.049712	4.798824
237.030341	7950.805254	9.225971	-0.049754	4.801194
237.065586	7958.778899	9.230976	-0.049766	4.803532
237.304754	7966.799027	9.235981	-0.049816	4.805881
237.697886	7974.850110	9.240986	-0.049895	4.808238
237.896610	7982.853156	9.245991	-0.049937	4.810580
237.931060	7990.395480	9.250995	-0.049949	4.812787
238.040303	7995.154122	9.256000	-0.049972	4.814178

238.011557	7997.675154	9.261005	-0.049969	4.814916
238.106262	7998.870332	9.266010	-0.049988	4.815265
237.942595	7999.564903	9.271015	-0.049958	4.815468
238.182679	7999.770629	9.276019	-0.050003	4.815528
238.359499	8000.266831	9.281024	-0.050036	4.815672
238.359199	8000.192104	9.286029	-0.050037	4.815650
238.536616	8000.158709	9.291034	-0.050070	4.815639
238.602157	8000.232407	9.296039	-0.050082	4.815660
238.514790	8000.168009	9.301043	-0.050066	4.815642
238.352250	8000.256147	9.306048	-0.050036	4.815669
238.467019	8000.262308	9.311053	-0.050058	4.815670
238.651421	8000.089148	9.316058	-0.050092	4.815618
238.592573	8000.260125	9.321063	-0.050082	4.815669
238.815305	8000.108944	9.326067	-0.050123	4.815623
238.856164	7999.988972	9.331072	-0.050131	4.815588
238.934093	8000.056465	9.336077	-0.050146	4.815607
239.169764	8000.153219	9.341082	-0.050190	4.815635
239.260701	8000.186755	9.346087	-0.050207	4.815644
239.169423	8000.146851	9.351091	-0.050191	4.815633
239.314003	8000.048855	9.356096	-0.050218	4.815603
239.313750	8000.222923	9.361101	-0.050218	4.815654
239.302215	8000.057250	9.366106	-0.050216	4.815606
239.128232	8000.271202	9.371111	-0.050184	4.815669
239.208782	8000.061113	9.376115	-0.050199	4.815607
239.387373	8000.051228	9.381120	-0.050233	4.815604
239.186212	8000.013808	9.386125	-0.050196	4.815594
239.414480	8000.084816	9.391130	-0.050238	4.815613
239.453981	8000.150616	9.396135	-0.050246	4.815632
239.491614	7999.912066	9.401139	-0.050253	4.815562
239.214546	8000.191611	9.406144	-0.050202	4.815646
239.243008	8000.230537	9.411149	-0.050208	4.815657
239.321440	8000.101566	9.416154	-0.050222	4.815619
239.457444	8000.268242	9.421159	-0.050248	4.815667
239.550836	8000.266582	9.426163	-0.050266	4.815666
239.568327	8000.168651	9.431168	-0.050269	4.815637
239.510844	8000.226467	9.436173	-0.050259	4.815654
239.418829	8000.068025	9.441178	-0.050242	4.815608
239.649445	8000.246920	9.446183	-0.050285	4.815660
239.578148	8000.239375	9.451187	-0.050272	4.815658
239.404343	8000.095619	9.456192	-0.050240	4.815616
239.363180	8000.153700	9.461197	-0.050232	4.815634
239.580591	8000.063295	9.466202	-0.050273	4.815606
239.475371	8000.294385	9.471207	-0.050254	4.815674
239.535319	7999.945146	9.476211	-0.050265	4.815572
239.723858	7999.989881	9.481216	-0.050300	4.815584
239.606426	8000.154568	9.486221	-0.050279	4.815633
239.446467	7999.976869	9.491226	-0.050249	4.815582
239.660286	8000.096760	9.496231	-0.050289	4.815616
239.774879	8000.093309	9.501235	-0.050311	4.815614
239.528490	8000.073304	9.506240	-0.050265	4.815609
239.503379	8000.245901	9.511245	-0.050261	4.815660
239.949203	7999.971281	9.516250	-0.050344	4.815577
239.896129	8000.086830	9.521255	-0.050335	4.815611
239.885018	8000.174231	9.526259	-0.050333	4.815637
239.768173	8000.193708	9.531264	-0.050311	4.815643
239.767137	8000.254578	9.536269	-0.050312	4.815661
239.795851	8000.004134	9.541274	-0.050317	4.815588
239.767510	8000.081644	9.546279	-0.050312	4.815611
239.851115	7999.957028	9.551283	-0.050328	4.815574
239.706532	8000.019832	9.556288	-0.050301	4.815593
239.735151	8000.193304	9.561293	-0.050307	4.815643
239.858398	7999.992450	9.566298	-0.050330	4.815584
239.762859	8000.182054	9.571303	-0.050312	4.815640
239.679276	8000.084614	9.576307	-0.050297	4.815612
239.853762	7999.990306	9.581312	-0.050330	4.815583
239.964492	7999.989995	9.586317	-0.050351	4.815583
239.880228	7999.997189	9.591322	-0.050335	4.815585
239.962910	8000.128829	9.596327	-0.050351	4.815623
240.073520	7999.960871	9.601331	-0.050372	4.815574
239.986951	8000.080146	9.606336	-0.050356	4.815609
239.930661	7999.976743	9.611341	-0.050346	4.815579
240.015079	8000.083852	9.616346	-0.050362	4.815610
239.930219	7999.969306	9.621351	-0.050346	4.815577
239.888918	7999.977198	9.626355	-0.050339	4.815579
239.874885	8000.046399	9.631360	-0.050336	4.815600
239.789884	8000.136869	9.636365	-0.050321	4.815626
239.995267	8000.077234	9.641370	-0.050359	4.815608
240.063195	8000.000413	9.646375	-0.050372	4.815585
240.134387	8000.038967	9.651379	-0.050386	4.815596
240.060186	8000.052731	9.656384	-0.050372	4.815601
240.080063	8000.104332	9.661389	-0.050376	4.815616
240.206219	7999.970796	9.666394	-0.050400	4.815576
240.078850	8000.115035	9.671399	-0.050376	4.815619
239.915917	8000.120947	9.676403	-0.050346	4.815621
240.385349	8000.069882	9.681408	-0.050434	4.815604
240.430169	8000.217994	9.686413	-0.050443	4.815647
240.376491	7999.974748	9.691418	-0.050433	4.815576
240.209439	8000.214444	9.696423	-0.050402	4.815647
240.280109	8000.050106	9.701427	-0.050415	4.815599
240.317205	8000.144700	9.706432	-0.050423	4.815626
240.017232	8000.089651	9.711437	-0.050367	4.815611
240.345886	8000.117448	9.716442	-0.050428	4.815618
240.292079	8000.330159	9.721447	-0.050419	4.815680
240.373101	8000.090173	9.726451	-0.050434	4.815610
240.336100	8000.141916	9.731456	-0.050427	4.815625
240.330995	7999.980615	9.736461	-0.050427	4.815578
240.284346	7999.989488	9.741466	-0.050418	4.815581
240.240389	8000.247206	9.746471	-0.050410	4.815656
240.399840	7999.927345	9.751475	-0.050440	4.815562
240.384471	8000.160968	9.756480	-0.050438	4.815631
240.343882	8000.220128	9.761485	-0.050430	4.815648
240.606919	7999.923308	9.766490	-0.050479	4.815560
240.646757	7999.930386	9.771495	-0.050487	4.815562
240.360714	7999.922548	9.776499	-0.050434	4.815561
240.520807	8000.018077	9.781504	-0.050464	4.815588
240.562333	8000.171474	9.786509	-0.050472	4.815633
240.493550	7999.820133	9.791514	-0.050460	4.815530
240.361538	8000.160774	9.796519	-0.050435	4.815631
240.587070	8000.018177	9.801523	-0.050478	4.815588
240.380590	7999.890972	9.806528	-0.050439	4.815552
240.308209	8000.088429	9.811533	-0.050426	4.815610
240.461804	7999.884864	9.816538	-0.050455	4.815549
240.459481	8000.171023	9.821543	-0.050455	4.815633
240.505946	7999.931543	9.826547	-0.050464	4.815563
240.382869	7999.949850	9.831552	-0.050441	4.815569
240.530770	8000.085757	9.836557	-0.050469	4.815608
240.565671	7999.953939	9.841562	-0.050476	4.815569
240.427135	7999.988011	9.846567	-0.050450	4.815580
240.594596	7999.984353	9.851571	-0.050482	4.815578
240.715249	8000.128361	9.856576	-0.050504	4.815619
240.379634	8000.211547	9.861581	-0.050442	4.815645
240.553539	7999.938904	9.866586	-0.050475	4.815565
240.452887	7999.935152	9.871591	-0.050456	4.815564
240.333658	8000.006912	9.876595	-0.050434	4.815586
240.384315	7999.939419	9.881600	-0.050444	4.815566
240.542087	8000.016757	9.886605	-0.050474	4.815587
240.717924	7999.895776	9.891610	-0.050506	4.815551
240.478560	7999.957038	9.896615	-0.050462	4.815570
240.528731	8000.035827	9.901619	-0.050472	4.815593
240.615293	7999.972122	9.906624	-0.050488	4.815574
240.498284	8000.203025	9.911629	-0.050467	4.815642
240.614144	7999.964674	9.916634	-0.050488	4.815572
240.541864	8000.073504	9.921639	-0.050475	4.815604
240.627736	7999.982025	9.926643	-0.050492	4.815577
240.714186	7999.987726	9.931648	-0.050508	4.815578
240.832693	8000.003560	9.936653	-0.050530	4.815582
240.864978	7999.893054	9.941658	-0.050536	4.815550
240.679401	7999.984023	9.946663	-0.050502	4.815577
240.591907	7999.955925	9.951667	-0.050486	4.815569
240.627011	7999.968265	9.956672	-0.050493	4.815573
240.505465	7999.990869	9.961677	-0.050471	4.815580
240.606850	7999.958372	9.966682	-0.050490	4.815570
240.577383	7999.961118	9.971687	-0.050484	4.815571
240.503920	7999.981300	9.976691	-0.050471	4.815577
240.450127	8000.055194	9.981696	-0.050461	4.815599
240.841990	7999.972968	9.986701	-0.050535	4.815573
240.918941	7999.878139	9.991706	-0.050549	4.815545
240.795764	7999.977599	9.996711	-0.050526	4.815575
240.859332	7999.851586	10.001715	-0.050538	4.815537
240.810606	8000.012056	10.006720	-0.050530	4.815585
240.701358	7999.941959	10.011725	-0.050510	4.815565
240.657088	7999.772546	10.016730	-0.050501	4.815515
240.717416	7999.905959	10.021735	-0.050513	4.815554
240.774170	7999.825751	10.026739	-0.050524	4.815530
240.942073	7999.897915	10.031744	-0.050555	4.815551
240.785922	7999.979753	10.036749	-0.050527	4.815575
240.884316	7999.858578	10.041754	-0.050545	4.815539
240.643135	8000.139782	10.046759	-0.050501	4.815623
240.765447	7999.936774	10.051763	-0.050524	4.815563
240.822145	8000.141675	10.056768	-0.050535	4.815622
240.665413	8000.097499	10.061773	-0.050506	4.815610
240.667692	7999.929910	10.066778	-0.050506	4.815561
240.706752	8000.069386	10.071783	-0.050514	4.815602
240.749258	7999.935554	10.076787	-0.050522	4.815562
240.608368	8000.028319	10.081792	-0.050496	4.815590
240.722477	7999.915942	10.086797	-0.050517	4.815557
241.013977	7999.975170	10.091802	-0.050572	4.815573
240.699959	7999.965808	10.096807	-0.050514	4.815572
240.857305	8000.045276	10.101811	-0.050543	4.815594
240.966142	8000.017171	10.106816	-0.050564	4.815585
240.907936	7999.937227	10.111821	-0.050553	4.815562
240.804791	7999.867229	10.116826	-0.050534	4.815542
240.697321	7999.895401	10.121831	-0.050514	4.815551
240.900485	7999.841069	10.126835	-0.050552	4.815534
240.863091	8000.027351	10.131840	-0.050546	4.815589
240.676952	7999.979494	10.136845	-0.050511	4.815576
240.950285	7999.929508	10.141850	-0.050563	4.815560
240.940779	7999.850357	10.146855	-0.050561	4.815537
240.894505	7999.976697	10.151859	-0.050553	4.815574
240.974967	7999.956673	10.156864	-0.050568	4.815567
241.080701	7999.991520	10.161869	-0.050588	4.815577
241.053190	7999.891786	10.166874	-0.050583	4.815548
241.153113	7999.977794	10.171879	-0.050602	4.815573
241.096259	7999.960873	10.176883	-0.050592	4.815568
241.046166	7999.860772	10.181888	-0.050582	4.815539
240.838954	8000.159615	10.186893	-0.050544	4.815627
241.064264	7999.833348	10.191898	-0.050586	4.815531
240.960784	8000.001469	10.196903	-0.050567	4.815581
240.937413	8000.036349	10.201907	-0.050563	4.815591
241.096637	8000.050711	10.206912	-0.050593	4.815594
241.278956	7999.993904	10.211917	-0.050627	4.815577
241.082426	7999.808128	10.216922	-0.050591	4.815523
241.042537	7999.891858	10.221927	-0.050584	4.815548
241.043345	7999.859859	10.226931	-0.050584	4.815539
241.191919	7999.953066	10.231936	-0.050612	4.815565
240.997472	8000.249984	10.236941	-0.050576	4.815653
241.085317	8000.044276	10.241946	-0.050593	4.815592
241.133152	8000.026925	10.246951	-0.050602	4.815587
241.103909	7999.935705	10.251955	-0.050597	4.815561
241.090896	7999.877853	10.256960	-0.050595	4.815544
241.113064	8000.165484	10.261965	-0.050599	4.815628
241.247299	7999.946650	10.266970	-0.050624	4.815563
241.055872	7999.979861	10.271975	-0.050589	4.815574
241.101050	7999.920821	10.276979	-0.050598	4.815556
241.083385	7999.829790	10.281984	-0.050594	4.815530
240.977899	7999.994676	10.286989	-0.050575	4.815578
241.163043	7999.968882	10.291994	-0.050610	4.815570
241.078334	7999.983542	10.296999	-0.050594	4.815575
241.016042	8000.030603	10.302003	-0.050583	4.815589
240.968367	7999.995678	10.307008	-0.050574	4.815579
241.080049	8000.142745	10.312013	-0.050596	4.815621
241.266525	7999.976018	10.317018	-0.050630	4.815572
241.150619	7999.951728	10.322023	-0.050609	4.815565
241.350474	7999.899478	10.327027	-0.050647	4.815549
241.327473	7999.895923	10.332032	-0.050643	4.815548
240.878476	8000.135302	10.337037	-0.050559	4.815620
240.995978	7999.824364	10.342042	-0.050581	4.815528
241.112323	7999.986455	10.347047	-0.050603	4.815575
241.093672	8000.080143	10.352051	-0.050600	4.815603
241.255492	7999.839335	10.357056	-0.050630	4.815532
241.376732	8000.039949	10.362061	-0.050653	4.815590
241.376541	7999.994051	10.367066	-0.050653	4.815576
241.250741	8000.191711	10.372071	-0.050630	4.815635
241.182101	8000.001608	10.377075	-0.050618	4.815579
241.079053	7999.888897	10.382080	-0.050599	4.815547
240.898883	7999.939377	10.387085	-0.050566	4.815562
241.166457	7999.843381	10.392090	-0.050616	4.815533
241.172393	7999.940672	10.397095	-0.050617	4.815562
241.119472	7999.960122	10.402099	-0.050607	4.815567
241.230169	7999.999321	10.407104	-0.050628	4.815578
241.432166	8000.121165	10.412109	-0.050666	4.815613
241.422718	7999.845530	10.417114	-0.050665	4.815532
241.239544	8000.095647	10.422119	-0.050631	4.815606
241.437565	7999.961143	10.427123	-0.050668	4.815566
241.544463	7999.858258	10.432128	-0.050688	4.815536
241.249772	7999.985893	10.437133	-0.050633	4.815574
241.342740	7999.850747	10.442138	-0.050651	4.815534
241.194575	8000.090755	10.447143	-0.050624	4.815605
241.248267	8000.024378	10.452147	-0.050634	4.815586
241.216951	8000.076214	10.457152	-0.050628	4.815601
241.138491	7999.989531	10.462157	-0.050614	4.815576
241.151960	7999.836006	10.467162	-0.050617	4.815531
241.234945	8000.150256	10.472167	-0.050633	4.815622
241.310681	8000.163258	10.477171	-0.050647	4.815626
241.087562	8000.104118	10.482176	-0.050606	4.815610
241.239189	8000.103407	10.487181	-0.050634	4.815609
241.344575	8000.013311	10.492186	-0.050654	4.815582
241.312401	7999.988249	10.497191	-0.050648	4.815575
241.276266	8000.211930	10.502195	-0.050642	4.815640
241.323318	7999.939351	10.507200	-0.050651	4.815560
241.490122	8000.190899	10.512205	-0.050682	4.815633
241.705046	7999.807862	10.517210	-0.050722	4.815520
241.435505	8000.145204	10.522215	-0.050672	4.815620
241.437548	7999.940233	10.527219	-0.050673	4.815560
241.379952	8000.022609	10.532224	-0.050663	4.815584
241.347487	7999.923861	10.537229	-0.050657	4.815556
241.431384	7999.880401	10.542234	-0.050673	4.815542
241.420902	8000.102364	10.547239	-0.050671	4.815607
241.432087	7999.837744	10.552243	-0.050673	4.815530
241.447765	7999.951212	10.557248	-0.050676	4.815563
241.404955	7999.940927	10.562253	-0.050669	4.815560
241.399240	7999.849022	10.567258	-0.050668	4.815533
241.377153	7999.846549	10.572263	-0.050664	4.815533
241.406318	7999.879082	10.577267	-0.050670	4.815542
241.517105	8000.049627	10.582272	-0.050691	4.815592
241.322694	8000.014448	10.587277	-0.050655	4.815582
241.470508	7999.950671	10.592282	-0.050682	4.815563
241.470758	7999.868474	10.597287	-0.050683	4.815539
241.489085	8000.003343	10.602291	-0.050686	4.815578
241.318724	7999.990980	10.607296	-0.050655	4.815575
241.458653	8000.046674	10.612301	-0.050681	4.815591
241.405000	7999.825847	10.617306	-0.050671	4.815527
241.354933	8000.220156	10.622311	-0.050663	4.815642
241.278830	8000.081186	10.627315	-0.050649	4.815602
241.387464	7999.968719	10.632320	-0.050669	4.815568
241.375092	7999.959997	10.637325	-0.050667	4.815566
241.539601	7999.961631	10.642330	-0.050698	4.815566
241.508344	7999.966484	10.647335	-0.050692	4.815567
241.443974	7999.851199	10.652339	-0.050681	4.815534
241.652543	7999.877043	10.657344	-0.050720	4.815540
241.374991	7999.995346	10.662349	-0.050668	4.815576
241.687901	7999.918241	10.667354	-0.050727	4.815552
241.680225	7999.885036	10.672359	-0.050726	4.815542
241.672801	7999.922312	10.677363	-0.050724	4.815553
241.706231	7999.821433	10.682368	-0.050731	4.815524
241.520275	7999.893176	10.687373	-0.050697	4.815546
241.482361	7999.831714	10.692378	-0.050690	4.815528
241.522981	7999.959471	10.697383	-0.050698	4.815565
241.577624	7999.831175	10.702387	-0.050708	4.815527
241.696853	7999.887599	10.707392	-0.050730	4.815543
241.565963	7999.967713	10.712397	-0.050706	4.815567
241.620040	7999.858628	10.717402	-0.050717	4.815535
241.627660	7999.864114	10.722407	-0.050718	4.815537
241.639565	7999.872873	10.727411	-0.050721	4.815539
241.864195	7999.868012	10.732416	-0.050763	4.815537
241.938651	7999.947200	10.737421	-0.050777	4.815559
241.846119	7999.846405	10.742426	-0.050760	4.815530
241.682210	7999.996460	10.747431	-0.050730	4.815575
241.785743	7999.851873	10.752435	-0.050749	4.815532
241.731149	7999.840328	10.757440	-0.050739	4.815529
241.559445	8000.039376	10.762445	-0.050708	4.815588
241.726531	7999.791177	10.767450	-0.050739	4.815515
241.686622	7999.820449	10.772455	-0.050732	4.815523
241.684384	7999.842859	10.777459	-0.050732	4.815530
241.493619	7999.844046	10.782464	-0.050696	4.815531
241.465858	7999.972825	10.787469	-0.050692	4.815569
241.561708	7999.852675	10.792474	-0.050710	4.815533
241.621850	7999.972207	10.797479	-0.050721	4.815568
241.682704	7999.835469	10.802483	-0.050733	4.815528
241.546757	7999.766004	10.807488	-0.050708	4.815508
241.449572	7999.924619	10.812493	-0.050690	4.815555
241.788981	7999.828724	10.817498	-0.050753	4.815525
241.797653	7999.997608	10.822503	-0.050755	4.815575
241.776797	7999.950305	10.827507	-0.050752	4.815561
242.023185	7999.934052	10.832512	-0.050798	4.815555
241.877404	7999.934903	10.837517	-0.050771	4.815556
241.987202	7999.856625	10.842522	-0.050791	4.815532
241.696152	8000.074020	10.847527	-0.050738	4.815597
241.763586	7999.958745	10.852531	-0.050750	4.815563
241.890847	7999.921330	10.857536	-0.050774	4.815552
241.804139	7999.997893	10.862541	-0.050758	4.815575
241.907415	8000.009208	10.867546	-0.050778	4.815577
241.769758	8000.024074	10.872551	-0.050753	4.815582
241.895143	7999.931100	10.877555	-0.050776	4.815555
241.881401	7999.857217	10.882560	-0.050774	4.815533
241.861638	8000.066216	10.887565	-0.050770	4.815594
241.857311	7999.817359	10.892570	-0.050770	4.815522
241.737626	7999.959591	10.897575	-0.050748	4.815564
242.021591	7999.843572	10.902579	-0.050801	4.815528
242.017505	7999.862749	10.907584	-0.050800	4.815534
241.693072	7999.924761	10.912589	-0.050740	4.815554
241.952301	7999.743201	10.917594	-0.050789	4.815499
241.833671	7999.995439	10.922599	-0.050767	4.815574
241.954854	7999.950450	10.927603	-0.050790	4.815560
241.742794	7999.867997	10.932608	-0.050751	4.815537
241.917052	7999.846297	10.937613	-0.050783	4.815530
242.024665	7999.935636	10.942618	-0.050804	4.815555
241.899755	8000.036138	10.947623	-0.050781	4.815585
241.911136	7999.955189	10.952627	-0.050783	4.815562
241.802415	7999.861605	10.957632	-0.050763	4.815535
241.713390	7999.859109	10.962637	-0.050747	4.815534
241.773639	7999.760804	10.967642	-0.050758	4.815505
241.676183	7999.839327	10.972647	-0.050740	4.815529
241.950274	7999.910020	10.977651	-0.050791	4.815548
241.938601	7999.873546	10.982656	-0.050790	4.815537
242.013113	7999.974093	10.987661	-0.050804	4.815567
242.097440	7999.830260	10.992666	-0.050820	4.815524
241.940825	7999.962281	10.997671	-0.050791	4.815563
242.122069	7999.980206	11.002675	-0.050825	4.815568
242.138981	7999.958079	11.007680	-0.050828	4.815561
241.844274	7999.940486	11.012685	-0.050774	4.815557
242.032316	7999.985218	11.017690	-0.050809	4.815570
241.998357	7999.976144	11.022695	-0.050803	4.815567
241.881440	7999.896309	11.027699	-0.050781	4.815544
241.894045	7999.922165	11.032704	-0.050784	4.815552
241.885782	7999.951952	11.037709	-0.050783	4.815561
242.019381	7999.839891	11.042714	-0.050808	4.815527
241.704634	7999.911671	11.047719	-0.050749	4.815550
241.862848	7999.930289	11.052723	-0.050779	4.815554
242.235902	7999.773007	11.057728	-0.050849	4.815507
241.938225	7999.982819	11.062733	-0.050794	4.815569
242.203411	7999.835526	11.067738	-0.050843	4.815525
242.309381	7999.877853	11.072743	-0.050863	4.815537
242.273839	7999.894382	11.077747	-0.050857	4.815542
242.197288	7999.853647	11.082752	-0.050843	4.815530
242.061241	7999.940085	11.087757	-0.050818	4.815556
242.036754	7999.867094	11.092762	-0.050813	4.815535
241.859260	7999.856750	11.097767	-0.050781	4.815533
242.049052	7999.917528	11.102771	-0.050816	4.815550
242.181642	7999.839622	11.107776	-0.050841	4.815526
242.030456	7999.932220	11.112781	-0.050813	4.815554
242.142613	7999.958631	11.117786	-0.050834	4.815561
242.216533	7999.913939	11.122791	-0.050848	4.815548
241.962120	7999.821185	11.127795	-0.050801	4.815522
242.056021	7999.883605	11.132800	-0.050819	4.815540
241.886815	7999.855242	11.137805	-0.050788	4.815532
242.106083	7999.773408	11.142810	-0.050829	4.815507
242.091042	7999.860750	11.147815	-0.050826	4.815533
242.030386	7999.934534	11.152819	-0.050815	4.815555
242.092547	7999.821308	11.157824	-0.050827	4.815521
242.212188	7999.969577	11.162829	-0.050850	4.815564
242.213157	7999.824386	11.167834	-0.050850	4.815522
242.274754	7999.939673	11.172839	-0.050862	4.815555
242.218262	7999.819174	11.177843	-0.050852	4.815520
242.330587	7999.947034	11.182848	-0.050873	4.815557
242.142827	7999.883129	11.187853	-0.050838	4.815539
242.031400	7999.836487	11.192858	-0.050818	4.815526
241.969497	7999.899572	11.197863	-0.050806	4.815545
241.855926	7999.836877	11.202867	-0.050785	4.815527
242.002659	7999.924717	11.207872	-0.050813	4.815552
241.782066	7999.810090	11.212877	-0.050772	4.815519
241.758964	7999.783040	11.217882	-0.050768	4.815512
241.863322	7999.896886	11.222887	-0.050788	4.815544
241.796946	7999.853113	11.227891	-0.050776	4.815532
241.957911	7999.834401	11.232896	-0.050806	4.815526
241.827582	7999.858996	11.237901	-0.050782	4.815533
241.978655	7999.754695	11.242906	-0.050810	4.815502
242.095127	7999.947760	11.247911	-0.050832	4.815558
242.010200	7999.859903	11.252915	-0.050817	4.815533
242.116829	7999.878748	11.257920	-0.050837	4.815538
242.089348	7999.845219	11.262925	-0.050832	4.815528
241.981028	7999.846680	11.267930	-0.050812	4.815529
242.021204	7999.952007	11.272935	-0.050820	4.815560
241.997159	7999.954841	11.277939	-0.050816	4.815561
241.832519	7999.849667	11.282944	-0.050785	4.815531
241.855168	7999.984608	11.287949	-0.050790	4.815570
242.102941	7999.760146	11.292954	-0.050836	4.815503
242.012402	7999.950908	11.297959	-0.050819	4.815559
241.929203	7999.758429	11.302963	-0.050804	4.815503
242.100550	7999.857349	11.307968	-0.050836	4.815532
241.789018	7999.991117	11.312973	-0.050779	4.815572
241.825307	7999.859317	11.317978	-0.050786	4.815533
241.943987	7999.885833	11.322983	-0.050808	4.815541
242.007428	7999.960572	11.327987	-0.050820	4.815562
242.128880	7999.793851	11.332992	-0.050843	4.815513
241.899438	7999.939635	11.337997	-0.050800	4.815557
242.252828	7999.748930	11.343002	-0.050866	4.815499
242.213594	7999.870048	11.348007	-0.050859	4.815535
242.024041	7999.913968	11.353011	-0.050824	4.815548
242.288658	7999.742105	11.358016	-0.050874	4.815497
241.933108	7999.966992	11.363021	-0.050808	4.815564
242.062730	7999.921073	11.368026	-0.050832	4.815550
241.906627	7999.891856	11.373031	-0.050804	4.815542
242.104110	7999.821413	11.378035	-0.050841	4.815521
242.054628	7999.876158	11.383040	-0.050832	4.815537
241.908221	7999.860981	11.388045	-0.050805	4.815533
242.060073	7999.863477	11.393050	-0.050833	4.815533
242.190096	7999.860279	11.398055	-0.050858	4.815532
241.979166	7999.776776	11.403059	-0.050818	4.815508
242.194669	7999.879619	11.408064	-0.050859	4.815537
242.241400	7999.855842	11.413069	-0.050868	4.815530
242.232984	7999.824760	11.418074	-0.050867	4.815521
242.094623	7999.808646	11.423079	-0.050841	4.815517
242.243163	7999.851667	11.428083	-0.050869	4.815529
242.432649	7999.835555	11.433088	-0.050905	4.815523
241.963105	8000.001988	11.438093	-0.050817	4.815574
242.140782	7999.781723	11.443098	-0.050851	4.815509
242.253373	7999.878619	11.448103	-0.050872	4.815537
241.975312	7999.880518	11.453107	-0.050820	4.815539
241.853763	7999.859339	11.458112	-0.050798	4.815533
242.048716	7999.920202	11.463117	-0.050835	4.815550
242.218389	7999.920853	11.468122	-0.050866	4.815549
242.184778	7999.790049	11.473127	-0.050860	4.815511
242.080392	7999.850306	11.478131	-0.050841	4.815529
242.098655	7999.861305	11.483136	-0.050845	4.815532
242.105541	7999.919104	11.488141	-0.050846	4.815549
242.203596	7999.910045	11.493146	-0.050865	4.815546
242.110886	7999.950204	11.498151	-0.050848	4.815558
242.160416	7999.972390	11.503155	-0.050857	4.815565
242.075449	7999.956078	11.508160	-0.050842	4.815560
241.987828	7999.949334	11.513165	-0.050826	4.815559
241.945149	7999.834400	11.518170	-0.050818	4.815525
242.004433	7999.862085	11.523175	-0.050829	4.815533
242.090422	7999.894476	11.528179	-0.050846	4.815542
242.248265	7999.794555	11.533184	-0.050875	4.815512
242.048537	7999.893838	11.538189	-0.050838	4.815542
242.117326	7999.862946	11.543194	-0.050851	4.815533
242.241682	7999.787040	11.548199	-0.050875	4.815510
242.150649	7999.954301	11.553203	-0.050858	4.815559
241.980302	7999.833016	11.558208	-0.050827	4.815525
242.059469	7999.823650	11.563213	-0.050842	4.815522
242.353165	7999.824185	11.568218	-0.050897	4.815520
242.210112	7999.928663	11.573223	-0.050870	4.815552
242.209054	8000.010894	11.578227	-0.050870	4.815576
242.197317	7999.910346	11.583232	-0.050868	4.815546
242.084750	7999.957656	11.588237	-0.050848	4.815561
242.186753	7999.928372	11.593242	-0.050867	4.815552
242.428695	7999.894962	11.598247	-0.050912	4.815541
242.417551	7999.977028	11.603251	-0.050910	4.815565
242.123188	7999.958372	11.608256	-0.050856	4.815561
242.318269	7999.960505	11.613261	-0.050892	4.815560
242.398258	7999.850773	11.618266	-0.050908	4.815528
242.208418	7999.917113	11.623271	-0.050873	4.815548
242.044190	7999.866406	11.628275	-0.050842	4.815534
242.340532	7999.822135	11.633280	-0.050898	4.815520
242.216973	7999.985663	11.638285	-0.050875	4.815568
242.213841	7999.874576	11.643290	-0.050875	4.815536
242.228287	7999.928227	11.648295	-0.050878	4.815551
242.369947	7999.833382	11.653299	-0.050904	4.815523
242.279471	7999.923767	11.658304	-0.050888	4.815550
242.273799	8000.104167	11.663309	-0.050887	4.815602
242.453568	7999.825201	11.668314	-0.050920	4.815520
242.242984	8000.024687	11.673319	-0.050882	4.815579
242.049093	7999.953206	11.678323	-0.050846	4.815559
242.225843	7999.825829	11.683328	-0.050879	4.815521
242.097375	8000.097132	11.688333	-0.050855	4.815601
242.176859	7999.907301	11.693338	-0.050870	4.815545
242.359009	7999.928445	11.698343	-0.050904	4.815551
242.338868	8000.080845	11.703347	-0.050901	4.815595
242.386336	7999.869135	11.708352	-0.050910	4.815533
242.342741	7999.858836	11.713357	-0.050902	4.815530
242.474481	7999.858869	11.718362	-0.050927	4.815530
242.339844	7999.841748	11.723367	-0.050902	4.815525
242.154066	8000.364138	11.728371	-0.050868	4.815679
242.485114	8000.029970	11.733376	-0.050930	4.815580
242.321463	8000.024121	11.738381	-0.050900	4.815579
242.372939	7999.894702	11.743386	-0.050909	4.815541
242.578026	7999.829723	11.748391	-0.050948	4.815521
242.345335	7999.863329	11.753395	-0.050905	4.815532
242.540030	7999.803520	11.758400	-0.050941	4.815513
242.145102	7999.901758	11.763405	-0.050868	4.815544
242.137586	7999.777786	11.768410	-0.050867	4.815508
242.036542	7999.938477	11.773415	-0.050848	4.815555
242.159533	7999.938367	11.778419	-0.050871	4.815554
242.379459	7999.870426	11.783424	-0.050913	4.815533
242.368902	7999.926874	11.788429	-0.050911	4.815550
242.293780	7999.844514	11.793434	-0.050897	4.815526
242.306662	7999.963280	11.798439	-0.050900	4.815561
242.281958	7999.944746	11.803443	-0.050895	4.815556
242.185243	7999.766995	11.808448	-0.050878	4.815504
242.093555	7999.979096	11.813453	-0.050861	4.815567
242.271221	7999.851734	11.818458	-0.050894	4.815528
242.238153	7999.850149	11.823463	-0.050888	4.815528
242.186789	7999.948646	11.828467	-0.050879	4.815557
242.484134	7999.902256	11.833472	-0.050935	4.815542
242.164436	7999.936580	11.838477	-0.050875	4.815554
241.999771	8000.025756	11.843482	-0.050845	4.815581
242.172598	7999.955979	11.848487	-0.050877	4.815559
242.251544	7999.949813	11.853491	-0.050892	4.815557
242.269470	7999.817712	11.858496	-0.050896	4.815518
242.198873	7999.827263	11.863501	-0.050883	4.815522
242.366841	7999.941081	11.868506	-0.050915	4.815554
242.170701	7999.875971	11.873511	-0.050878	4.815536
242.032015	7999.907905	11.878515	-0.050853	4.815546
242.159328	7999.930291	11.883520	-0.050877	4.815552
242.226501	7999.934612	11.888525	-0.050889	4.815553
242.289694	7999.833149	11.893530	-0.050901	4.815523
242.075045	7999.861710	11.898535	-0.050862	4.815532
242.289909	7999.975223	11.903539	-0.050902	4.815564
242.553396	7999.834309	11.908544	-0.050951	4.815522
242.361520	7999.973231	11.913549	-0.050916	4.815563
242.511069	7999.855021	11.918554	-0.050944	4.815528
242.355022	7999.832212	11.923559	-0.050915	4.815522
242.160230	7999.920896	11.928563	-0.050879	4.815549
242.458590	7999.884134	11.933568	-0.050935	4.815537
242.269273	7999.845832	11.938573	-0.050900	4.815527
242.063890	7999.839304	11.943578	-0.050862	4.815526
242.153453	7999.861075	11.948583	-0.050879	4.815532
242.138480	7999.951622	11.953587	-0.050876	4.815558
242.323362	7999.768849	11.958592	-0.050911	4.815504
242.183224	7999.960939	11.963597	-0.050885	4.815561
242.285739	7999.740516	11.968602	-0.050904	4.815496
242.254427	7999.910886	11.973607	-0.050899	4.815546
242.298580	7999.830470	11.978611	-0.050907	4.815522
242.466187	7999.747794	11.983616	-0.050939	4.815497
242.404247	7999.948635	11.988621	-0.050928	4.815556
242.533341	7999.881349	11.993626	-0.050952	4.815536
242.376785	7999.861734	11.998631	-0.050923	4.815531
242.504132	7999.919361	12.003635	-0.050947	4.815547
242.555864	8000.008861	12.008640	-0.050957	4.815573
242.373141	8000.025127	12.013645	-0.050923	4.815578
242.619698	7999.893547	12.018650	-0.050969	4.815539
242.589572	7999.912300	12.023655	-0.050964	4.815544
242.320564	7999.857749	12.028659	-0.050914	4.815530
242.528169	7999.791743	12.033664	-0.050953	4.815509
242.641782	7999.948458	12.038669	-0.050974	4.815555
242.403110	7999.886926	12.043674	-0.050930	4.815538
242.421553	7999.943846	12.048679	-0.050934	4.815554
242.471690	7999.852848	12.053683	-0.050943	4.815528
242.537870	7999.841135	12.058688	-0.050956	4.815524
242.422878	7999.855301	12.063693	-0.050935	4.815528
242.339040	7999.740764	12.068698	-0.050919	4.815495
242.552092	7999.877741	12.073703	-0.050960	4.815534
242.672631	7999.844488	12.078707	-0.050982	4.815524
242.709748	7999.813079	12.083712	-0.050989	4.815515
242.447579	8000.065119	12.088717	-0.050941	4.815590
242.523519	7999.862415	12.093722	-0.050955	4.815530
242.560969	7999.855572	12.098727	-0.050962	4.815528
242.615107	7999.961129	12.103731	-0.050973	4.815558
242.600687	7999.841314	12.108736	-0.050970	4.815523
242.479295	7999.962164	12.113741	-0.050948	4.815559
242.556920	7999.764827	12.118746	-0.050963	4.815501
242.483213	7999.809567	12.123751	-0.050949	4.815515
242.311842	7999.950959	12.128755	-0.050918	4.815557
242.467761	7999.831785	12.133760	-0.050947	4.815521
242.547763	7999.980478	12.138765	-0.050962	4.815564
242.736361	7999.836207	12.143770	-0.050997	4.815521
242.665113	7999.822254	12.148775	-0.050984	4.815518
242.638701	8000.142210	12.153779	-0.050980	4.815611
242.737413	7999.825612	12.158784	-0.050998	4.815518
242.545057	7999.936763	12.163789	-0.050963	4.815552
242.729168	7999.742229	12.168794	-0.050997	4.815494
242.703836	7999.865712	12.173799	-0.050993	4.815530
242.679103	7999.833295	12.178803	-0.050988	4.815521
242.745317	7999.901672	12.183808	-0.051001	4.815540
242.614258	7999.760735	12.188813	-0.050977	4.815500
242.646353	7999.846710	12.193818	-0.050983	4.815525
242.588080	7999.830833	12.198823	-0.050973	4.815520
242.607455	7999.935823	12.203827	-0.050977	4.815551
242.746332	7999.887918	12.208832	-0.051003	4.815536
242.582280	7999.876724	12.213837	-0.050972	4.815534
242.495789	7999.928731	12.218842	-0.050956	4.815549
242.604031	7999.846155	12.223847	-0.050977	4.815525
242.529156	7999.835346	12.228851	-0.050963	4.815522
242.765403	7999.790096	12.233856	-0.051007	4.815508
242.687763	7999.873216	12.238861	-0.050993	4.815532
242.678145	7999.826095	12.243866	-0.050992	4.815518
242.406930	7999.893245	12.248871	-0.050941	4.815539
242.470524	7999.849453	12.253875	-0.050954	4.815526
242.680552	7999.810183	12.258880	-0.050993	4.815514
242.480726	7999.862478	12.263885	-0.050956	4.815530
242.552745	7999.792127	12.268890	-0.050970	4.815509
242.544928	7999.934049	12.273895	-0.050968	4.815551
242.622209	7999.939603	12.278899	-0.050983	4.815552
242.583355	7999.877055	12.283904	-0.050976	4.815534
242.667769	7999.970291	12.288909	-0.050992	4.815561
242.815971	7999.862737	12.293914	-0.051020	4.815528
242.634865	7999.791464	12.298919	-0.050986	4.815508
242.560698	7999.847943	12.303923	-0.050973	4.815525
242.650662	7999.852635	12.308928	-0.050990	4.815526
242.480401	7999.878715	12.313933	-0.050958	4.815535
242.693730	7999.854449	12.318938	-0.050998	4.815527
242.819658	7999.898171	12.323943	-0.051022	4.815539
242.665235	7999.838012	12.328947	-0.050994	4.815522
242.454725	7999.769464	12.333952	-0.050955	4.815503
242.513290	7999.897517	12.338957	-0.050966	4.815540
242.643656	7999.788605	12.343962	-0.050990	4.815508
242.583015	7999.910445	12.348967	-0.050979	4.815543
242.505020	7999.930553	12.353971	-0.050965	4.815550
242.723022	7999.843359	12.358976	-0.051006	4.815523
242.639286	7999.924243	12.363981	-0.050991	4.815547
242.731873	7999.830734	12.368986	-0.051008	4.815519
242.779955	7999.765331	12.373991	-0.051017	4.815500
242.639724	7999.819666	12.378995	-0.050991	4.815517
242.746993	7999.925021	12.384000	-0.051012	4.815547
242.762883	8000.000054	12.389005	-0.051015	4.815569
242.925236	7999.816911	12.394010	-0.051045	4.815514
242.667002	7999.842625	12.399015	-0.050998	4.815523
242.604740	7999.881144	12.404019	-0.050986	4.815535
242.799540	7999.903563	12.409024	-0.051023	4.815540
242.716215	7999.829612	12.414029	-0.051007	4.815519
242.647430	7999.912876	12.419034	-0.050995	4.815544
242.543309	7999.904794	12.424039	-0.050976	4.815542
242.569438	7999.846509	12.429043	-0.050981	4.815525
242.517804	7999.842486	12.434048	-0.050972	4.815524
242.502839	7999.953324	12.439053	-0.050969	4.815556
242.579143	7999.931096	12.444058	-0.050984	4.815549
242.733944	7999.869569	12.449063	-0.051013	4.815531
242.450146	7999.946125	12.454067	-0.050960	4.815554
242.640989	7999.796551	12.459072	-0.050996	4.815510
242.699367	7999.835968	12.464077	-0.051007	4.815521
242.640335	7999.849979	12.469082	-0.050996	4.815525
242.727701	7999.788421	12.474087	-0.051013	4.815507
242.897603	7999.828588	12.479091	-0.051045	4.815518
242.943934	7999.874216	12.484096	-0.051053	4.815531
242.516585	7999.871545	12.489101	-0.050974	4.815532
242.828863	7999.832874	12.494106	-0.051032	4.815519
242.887350	8000.005779	12.499111	-0.051044	4.815570
242.757705	7999.827487	12.504115	-0.051020	4.815518
242.976332	7999.860974	12.509120	-0.051061	4.815527
242.867807	7999.891264	12.514125	-0.051041	4.815536
242.769968	7999.787175	12.519130	-0.051023	4.815506
242.630093	7999.979272	12.524135	-0.050997	4.815563
242.531458	7999.840998	12.529139	-0.050979	4.815523
242.701150	7999.836311	12.534144	-0.051011	4.815521
242.730737	7999.845358	12.539149	-0.051017	4.815523
242.923105	7999.978798	12.544154	-0.051053	4.815562
242.748154	7999.802972	12.549159	-0.051020	4.815511
242.452643	7999.850504	12.554163	-0.050966	4.815526
242.707239	7999.794875	12.559168	-0.051013	4.815509
242.736538	7999.871194	12.564173	-0.051019	4.815531
242.741119	7999.839255	12.569178	-0.051020	4.815522
242.605128	7999.887251	12.574183	-0.050995	4.815536
242.703654	7999.840825	12.579187	-0.051014	4.815522
242.731209	7999.839160	12.584192	-0.051019	4.815522
242.568883	7999.858963	12.589197	-0.050989	4.815528
242.766223	7999.821622	12.594202	-0.051026	4.815516
242.834279	7999.872944	12.599207	-0.051039	4.815531
242.702135	7999.944496	12.604211	-0.051015	4.815552
242.803285	7999.844718	12.609216	-0.051034	4.815523
242.757755	7999.945448	12.614221	-0.051025	4.815552
242.720353	7999.819918	12.619226	-0.051019	4.815516
242.593089	7999.874464	12.624231	-0.050995	4.815532
242.617669	7999.839647	12.629235	-0.051000	4.815522
242.682259	7999.803346	12.634240	-0.051012	4.815511
242.694658	7999.887933	12.639245	-0.051015	4.815536
242.939385	7999.874858	12.644250	-0.051061	4.815531
242.911841	7999.844531	12.649255	-0.051056	4.815522
242.688820	7999.847326	12.654259	-0.051015	4.815524
242.802166	7999.750951	12.659264	-0.051036	4.815495
242.958113	8000.035437	12.664269	-0.051065	4.815578
242.833494	7999.895670	12.669274	-0.051042	4.815537
242.670285	8000.017975	12.674279	-0.051012	4.815574
242.651127	7999.971766	12.679283	-0.051009	4.815561
242.803690	7999.816228	12.684288	-0.051038	4.815514
242.523795	7999.870422	12.689293	-0.050986	4.815532
242.626929	7999.952216	12.694298	-0.051005	4.815555
242.892071	7999.899963	12.699303	-0.051055	4.815538
242.681284	7999.977709	12.704307	-0.051016	4.815562
242.871174	7999.935975	12.709312	-0.051051	4.815549
242.809749	7999.839954	12.714317	-0.051040	4.815521
242.831968	7999.948195	12.719322	-0.051045	4.815553
242.793425	7999.886720	12.724327	-0.051038	4.815535
242.896682	7999.858525	12.729331	-0.051057	4.815526
242.871776	7999.785525	12.734336	-0.051053	4.815505
242.745616	7999.906298	12.739341	-0.051030	4.815541
242.935793	7999.774867	12.744346	-0.051065	4.815502
242.892367	7999.873494	12.749351	-0.051057	4.815531
242.693424	7999.845713	12.754355	-0.051021	4.815523
242.749276	7999.843442	12.759360	-0.051031	4.815523
242.731357	7999.832493	12.764365	-0.051028	4.815519
242.713012	7999.846099	12.769370	-0.051025	4.815523
242.659208	7999.796122	12.774375	-0.051015	4.815509
242.561774	7999.853290	12.779379	-0.050997	4.815526
242.894216	7999.794658	12.784384	-0.051059	4.815508
242.981830	7999.864453	12.789389	-0.051076	4.815528
242.860460	7999.956471	12.794394	-0.051054	4.815555
243.045585	7999.846315	12.799399	-0.051088	4.815522
242.840656	8000.054439	12.804403	-0.051051	4.815584
242.772682	7999.861133	12.809408	-0.051038	4.815528
242.960139	7999.945371	12.814413	-0.051073	4.815551
242.801948	7999.928932	12.819418	-0.051044	4.815547
242.850633	7999.930816	12.824423	-0.051053	4.815547
242.835169	7999.824865	12.829427	-0.051051	4.815517
242.861325	7999.848808	12.834432	-0.051056	4.815523
242.721928	7999.866848	12.839437	-0.051030	4.815529
242.896563	7999.864377	12.844442	-0.051063	4.815528
242.841078	7999.807965	12.849447	-0.051053	4.815512
242.683418	7999.864151	12.854451	-0.051024	4.815529
242.673564	7999.742275	12.859456	-0.051022	4.815493
242.691072	7999.879271	12.864461	-0.051026	4.815533
242.812577	7999.869527	12.869466	-0.051049	4.815530
242.854862	7999.858492	12.874471	-0.051057	4.815526
242.641969	8000.029110	12.879475	-0.051018	4.815577
242.884154	7999.836589	12.884480	-0.051063	4.815520
242.841659	7999.960861	12.889485	-0.051055	4.815556
242.603133	7999.857683	12.894490	-0.051011	4.815527
242.731337	7999.895035	12.899495	-0.051035	4.815537
242.886527	7999.871957	12.904499	-0.051064	4.815530
242.796746	7999.816054	12.909504	-0.051048	4.815514
242.672656	7999.787357	12.914509	-0.051025	4.815506
242.778476	7999.887349	12.919514	-0.051045	4.815535
242.782406	7999.794530	12.924519	-0.051046	4.815508
242.840619	7999.836081	12.929523	-0.051057	4.815520
242.958325	7999.871126	12.934528	-0.051079	4.815529
242.840526	7999.848939	12.939533	-0.051057	4.815523
242.871726	7999.861216	12.944538	-0.051064	4.815527
243.033604	7999.768835	12.949543	-0.051094	4.815499
243.000563	7999.984033	12.954547	-0.051088	4.815562
243.028503	7999.782680	12.959552	-0.051093	4.815503
243.091537	7999.876636	12.964557	-0.051105	4.815530
243.188940	7999.881450	12.969562	-0.051124	4.815531
243.281535	7999.793278	12.974567	-0.051141	4.815505
243.109714	7999.875931	12.979571	-0.051110	4.815530
243.203502	7999.843310	12.984576	-0.051127	4.815520
243.198816	7999.779183	12.989581	-0.051127	4.815501
242.940871	7999.834802	12.994586	-0.051079	4.815519
243.045075	7999.895257	12.999591	-0.051099	4.815536
242.865616	7999.869928	13.004595	-0.051065	4.815529
242.850387	7999.793883	13.009600	-0.051063	4.815507
242.689978	7999.962152	13.014605	-0.051033	4.815557
242.870664	7999.817752	13.019610	-0.051067	4.815514
243.048676	7999.853780	13.024615	-0.051101	4.815524
242.748138	7999.945013	13.029619	-0.051045	4.815552
243.005611	7999.740995	13.034624	-0.051093	4.815491
242.966841	7999.976389	13.039629	-0.051086	4.815560
242.981601	7999.865591	13.044634	-0.051089	4.815528
242.910323	7999.897556	13.049639	-0.051076	4.815537
243.042823	7999.957405	13.054643	-0.051101	4.815554
243.040948	7999.861286	13.059648	-0.051101	4.815526
242.950617	7999.835274	13.064653	-0.051084	4.815519
243.100445	7999.839875	13.069658	-0.051112	4.815519
243.077897	7999.789339	13.074663	-0.051108	4.815505
242.761234	7999.951858	13.079667	-0.051050	4.815554
242.957863	7999.900623	13.084672	-0.051087	4.815538
242.870070	7999.845820	13.089677	-0.051071	4.815522
242.827469	8000.329975	13.094682	-0.051063	4.815664
242.989136	8000.140410	13.099687	-0.051093	4.815608
243.134719	7999.987960	13.104691	-0.051121	4.815562
243.323721	7999.840490	13.109696	-0.051156	4.815518
243.101374	7999.942609	13.114701	-0.051115	4.815549
243.107653	7999.896815	13.119706	-0.051116	4.815536
243.326928	7999.865171	13.124711	-0.051157	4.815526
243.411260	7999.996853	13.129715	-0.051174	4.815564
243.417921	7999.767385	13.134720	-0.051175	4.815497
243.196289	7999.994460	13.139725	-0.051134	4.815564
243.136002	7999.865352	13.144730	-0.051123	4.815527
243.292102	7999.881802	13.149735	-0.051152	4.815531
243.235004	7999.949239	13.154739	-0.051142	4.815551
243.397226	7999.781042	13.159744	-0.051172	4.815501
243.157537	8000.002484	13.164749	-0.051128	4.815567
243.039445	7999.921556	13.169754	-0.051106	4.815543
243.209826	7999.922220	13.174759	-0.051138	4.815543
242.882731	7999.816529	13.179763	-0.051078	4.815513
243.044029	7999.785008	13.184768	-0.051108	4.815503
243.039711	7999.885342	13.189773	-0.051107	4.815533
243.282548	7999.843403	13.194778	-0.051153	4.815519
243.051035	7999.787325	13.199783	-0.051110	4.815504
243.021216	7999.838120	13.204787	-0.051105	4.815519
243.233227	7999.801018	13.209792	-0.051144	4.815507
242.872493	7999.942529	13.214797	-0.051078	4.815550
242.907211	7999.855551	13.219802	-0.051084	4.815525
243.203651	7999.880696	13.224807	-0.051140	4.815531
243.094720	7999.757203	13.229811	-0.051120	4.815495
243.067458	7999.915896	13.234816	-0.051115	4.815542
242.958980	7999.842602	13.239821	-0.051095	4.815521
242.932806	7999.855012	13.244826	-0.051090	4.815524
242.919898	7999.804633	13.249831	-0.051088	4.815510
242.915857	7999.870799	13.254835	-0.051088	4.815529
243.003488	7999.763325	13.259840	-0.051104	4.815497
242.873706	7999.871224	13.264845	-0.051080	4.815529
242.960553	7999.890817	13.269850	-0.051097	4.815535
243.196211	7999.803910	13.274855	-0.051141	4.815508
243.110358	7999.973396	13.279859	-0.051125	4.815558
243.087173	7999.850232	13.284864	-0.051121	4.815522
243.219834	7999.886590	13.289869	-0.051146	4.815532
243.118815	7999.890305	13.294874	-0.051127	4.815534
243.168260	7999.832399	13.299879	-0.051137	4.815517
243.041430	7999.792978	13.304883	-0.051113	4.815506
243.033451	7999.906067	13.309888	-0.051112	4.815539
242.921052	7999.800672	13.314893	-0.051092	4.815508
242.893766	7999.846168	13.319898	-0.051087	4.815522
242.844467	7999.878492	13.324903	-0.051078	4.815532
242.800636	7999.830813	13.329907	-0.051070	4.815518
242.827106	7999.780008	13.334912	-0.051075	4.815503
242.872060	7999.867262	13.339917	-0.051084	4.815528
242.987704	7999.765584	13.344922	-0.051105	4.815498
243.061213	7999.845829	13.349927	-0.051119	4.815521
242.938409	7999.838510	13.354931	-0.051097	4.815519
242.994149	7999.860798	13.359936	-0.051108	4.815526
242.961093	7999.923288	13.364941	-0.051102	4.815544
242.964584	7999.783473	13.369946	-0.051102	4.815503
243.302475	7999.889386	13.374951	-0.051166	4.815532
243.146896	7999.964829	13.379955	-0.051137	4.815555
243.065958	7999.807619	13.384960	-0.051122	4.815510
243.129217	7999.897307	13.389965	-0.051134	4.815536
243.329222	7999.862146	13.394970	-0.051172	4.815524
243.234355	7999.784801	13.399975	-0.051154	4.815502
243.094057	7999.865832	13.404979	-0.051128	4.815527
243.223447	7999.841267	13.409984	-0.051153	4.815519
243.196715	7999.938032	13.414989	-0.051148	4.815547
243.250433	7999.766999	13.419994	-0.051158	4.815497
243.179324	7999.885466	13.424999	-0.051145	4.815532
242.969873	7999.866056	13.430003	-0.051107	4.815527
243.027416	7999.799739	13.435008	-0.051118	4.815508
243.256515	7999.887860	13.440013	-0.051160	4.815532
243.021537	7999.856286	13.445018	-0.051117	4.815524
243.252840	7999.905999	13.450023	-0.051160	4.815537
242.946041	7999.832674	13.455027	-0.051103	4.815518
243.091872	7999.841481	13.460032	-0.051131	4.815519
243.119068	7999.882527	13.465037	-0.051136	4.815531
243.154621	7999.848957	13.470042	-0.051143	4.815521
243.338250	7999.866923	13.475047	-0.051177	4.815526
243.352995	7999.865050	13.480051	-0.051180	4.815525
243.317042	7999.879437	13.485056	-0.051174	4.815529
243.281511	7999.870337	13.490061	-0.051168	4.815527
243.360614	7999.856698	13.495066	-0.051183	4.815523
243.330814	7999.902155	13.500071	-0.051177	4.815536
243.123997	7999.878515	13.505075	-0.051139	4.815530
243.176683	7999.852699	13.510080	-0.051149	4.815522
243.205526	7999.857463	13.515085	-0.051155	4.815523
243.044879	7999.876225	13.520090	-0.051125	4.815530
243.002923	7999.884106	13.525095	-0.051118	4.815532
243.094223	7999.963574	13.530099	-0.051135	4.815555
243.229474	7999.866486	13.535104	-0.051160	4.815526
243.021643	7999.885546	13.540109	-0.051122	4.815532
243.211345	7999.852353	13.545114	-0.051157	4.815522
243.318682	7999.908588	13.550119	-0.051178	4.815538
243.046508	7999.867865	13.555123	-0.051127	4.815527
243.179105	7999.840148	13.560128	-0.051152	4.815518
243.089452	7999.837641	13.565133	-0.051136	4.815518
243.223333	7999.847321	13.570138	-0.051161	4.815520
243.341084	7999.906930	13.575143	-0.051183	4.815537
243.074879	7999.867371	13.580147	-0.051134	4.815527
242.985020	7999.871268	13.585152	-0.051117	4.815528
242.905371	7999.877467	13.590157	-0.051103	4.815531
243.286931	7999.864488	13.595162	-0.051174	4.815525
243.254706	7999.891751	13.600167	-0.051168	4.815533
242.967731	7999.873212	13.605171	-0.051115	4.815529
243.267508	7999.835405	13.610176	-0.051171	4.815517
243.304648	7999.812539	13.615181	-0.051178	4.815510
243.165378	7999.861550	13.620186	-0.051153	4.815525
243.126233	7999.844916	13.625191	-0.051146	4.815520
243.071179	7999.957238	13.630195	-0.051136	4.815553
243.053436	7999.806398	13.635200	-0.051133	4.815509
242.951916	7999.945727	13.640205	-0.051114	4.815550
243.075258	7999.837767	13.645210	-0.051137	4.815518
243.162359	7999.874450	13.650215	-0.051154	4.815528
242.794993	7999.859941	13.655219	-0.051086	4.815526
243.260586	7999.865418	13.660224	-0.051172	4.815525
243.137217	7999.869836	13.665229	-0.051150	4.815527
243.091886	7999.876595	13.670234	-0.051142	4.815529
243.376810	7999.838546	13.675239	-0.051195	4.815517
243.315270	7999.872806	13.680243	-0.051184	4.815527
243.277083	7999.874342	13.685248	-0.051177	4.815528
243.228207	7999.890654	13.690253	-0.051168	4.815533
242.966691	7999.858647	13.695258	-0.051120	4.815525
243.162513	7999.813807	13.700263	-0.051156	4.815511
243.015249	7999.878706	13.705267	-0.051129	4.815530
243.358166	7999.806362	13.710272	-0.051193	4.815508
243.464990	7999.956565	13.715277	-0.051213	4.815551
243.254632	7999.844231	13.720282	-0.051174	4.815519
243.222680	7999.890720	13.725287	-0.051169	4.815533
243.095501	7999.801102	13.730291	-0.051145	4.815507
243.270433	7999.886204	13.735296	-0.051178	4.815531
243.170302	7999.958279	13.740301	-0.051160	4.815553
243.175405	7999.746941	13.745306	-0.051161	4.815491
243.441618	7999.897606	13.750311	-0.051211	4.815534
242.992182	7999.858264	13.755315	-0.051127	4.815524
243.180402	7999.769515	13.760320	-0.051163	4.815498
243.270546	7999.954686	13.765325	-0.051180	4.815551
243.273307	7999.761464	13.770330	-0.051180	4.815495
243.108283	7999.893351	13.775335	-0.051150	4.815534
243.123873	7999.881880	13.780339	-0.051153	4.815531
243.401698	7999.791389	13.785344	-0.051205	4.815503
243.095139	7999.866506	13.790349	-0.051148	4.815526
243.105326	7999.886985	13.795354	-0.051150	4.815532
243.368698	7999.876351	13.800359	-0.051200	4.815528
242.959021	7999.869694	13.805363	-0.051124	4.815528
243.074807	7999.779765	13.810368	-0.051146	4.815501
243.271965	7999.891927	13.815373	-0.051183	4.815533
243.028401	7999.843127	13.820378	-0.051137	4.815520
243.058296	7999.884216	13.825383	-0.051143	4.815532
243.137370	7999.953874	13.830387	-0.051158	4.815552
243.159917	7999.781264	13.835392	-0.051163	4.815501
243.053745	7999.864987	13.840397	-0.051143	4.815526
243.122152	7999.778557	13.845402	-0.051156	4.815500
243.299401	7999.942723	13.850407	-0.051189	4.815547
243.208730	7999.864378	13.855411	-0.051173	4.815525
243.176837	7999.841454	13.860416	-0.051167	4.815518
243.330126	7999.972124	13.865421	-0.051196	4.815556
243.274409	7999.862312	13.870426	-0.051186	4.815524
243.330500	7999.791699	13.875431	-0.051196	4.815503
243.177316	7999.893879	13.880435	-0.051168	4.815534
243.309240	7999.856540	13.885440	-0.051193	4.815522
243.218850	7999.922366	13.890445	-0.051177	4.815542
243.102468	7999.861756	13.895450	-0.051155	4.815525
243.338180	7999.789801	13.900455	-0.051199	4.815503
243.262003	7999.851587	13.905459	-0.051185	4.815521
243.260233	7999.800322	13.910464	-0.051185	4.815506
243.303439	7999.885413	13.915469	-0.051194	4.815531
243.098591	7999.860737	13.920474	-0.051156	4.815524
243.004863	7999.944663	13.925479	-0.051138	4.815549
242.984351	7999.941148	13.930483	-0.051135	4.815548
243.226507	7999.787069	13.935488	-0.051180	4.815502
243.322014	7999.922136	13.940493	-0.051198	4.815541
243.268250	7999.875362	13.945498	-0.051188	4.815528
243.217686	7999.827573	13.950503	-0.051179	4.815514
243.271547	7999.885072	13.955507	-0.051190	4.815531
243.239894	7999.793807	13.960512	-0.051184	4.815504
243.291068	7999.877960	13.965517	-0.051194	4.815528
243.388176	7999.877430	13.970522	-0.051212	4.815528
243.358570	7999.882309	13.975527	-0.051207	4.815529
243.177628	7999.831325	13.980531	-0.051173	4.815515
243.248491	7999.866676	13.985536	-0.051187	4.815525
243.108027	7999.919939	13.990541	-0.051161	4.815542
243.061191	7999.862599	13.995546	-0.051152	4.815525
243.253655	7999.886050	14.000551	-0.051189	4.815531
243.183276	7999.893468	14.005555	-0.051176	4.815533
242.933151	7999.750586	14.010560	-0.051129	4.815493
242.944600	7999.904572	14.015565	-0.051132	4.815538
243.126272	7999.882994	14.020570	-0.051166	4.815531
243.198758	7999.791291	14.025575	-0.051180	4.815503
242.934298	7999.979224	14.030579	-0.051131	4.815560
243.194503	7999.773112	14.035584	-0.051179	4.815498
243.147039	7999.992349	14.040589	-0.051171	4.815562
243.074889	7999.876929	14.045594	-0.051158	4.815529
243.202785	7999.822438	14.050599	-0.051182	4.815513
243.048025	7999.776154	14.055603	-0.051153	4.815500
243.078575	7999.877056	14.060608	-0.051159	4.815529
243.174830	7999.873309	14.065613	-0.051177	4.815528
243.221329	7999.840984	14.070618	-0.051186	4.815518
243.321409	7999.941954	14.075623	-0.051205	4.815547
243.107493	7999.880821	14.080627	-0.051165	4.815530
243.217822	7999.792939	14.085632	-0.051186	4.815504
243.077939	7999.912421	14.090637	-0.051161	4.815539
242.992085	7999.932402	14.095642	-0.051145	4.815546
243.282993	7999.816494	14.100647	-0.051199	4.815510
243.327030	7999.896259	14.105651	-0.051208	4.815533
243.310152	7999.790284	14.110656	-0.051205	4.815503
243.119218	7999.869422	14.115661	-0.051169	4.815527
243.444849	7999.855532	14.120666	-0.051230	4.815521
243.534101	7999.898658	14.125671	-0.051247	4.815533
243.338292	7999.963833	14.130675	-0.051211	4.815553
243.451727	7999.849303	14.135680	-0.051232	4.815519
243.494627	7999.962156	14.140685	-0.051241	4.815552
243.243141	7999.864102	14.145690	-0.051194	4.815524
243.341046	7999.890282	14.150695	-0.051213	4.815532
243.416500	7999.871245	14.155699	-0.051227	4.815526
243.346188	7999.874392	14.160704	-0.051214	4.815527
243.262459	7999.893340	14.165709	-0.051199	4.815533
243.224960	7999.855374	14.170714	-0.051192	4.815522
243.267470	7999.787744	14.175719	-0.051200	4.815502
243.248954	7999.962601	14.180723	-0.051197	4.815553
243.308506	7999.816223	14.185728	-0.051208	4.815510
243.318218	7999.912515	14.190733	-0.051210	4.815538
243.130517	7999.831520	14.195738	-0.051176	4.815515
243.368613	7999.856783	14.200743	-0.051220	4.815522
243.509807	7999.895416	14.205747	-0.051247	4.815532
243.528964	7999.838084	14.210752	-0.051251	4.815515
243.202855	7999.922493	14.215757	-0.051190	4.815542
243.280072	7999.886398	14.220762	-0.051205	4.815531
243.640099	7999.835692	14.225767	-0.051272	4.815514
243.438870	7999.877285	14.230771	-0.051235	4.815527
243.357899	7999.856765	14.235776	-0.051220	4.815522
243.431856	7999.861197	14.240781	-0.051234	4.815523
243.255368	7999.870088	14.245786	-0.051201	4.815526
243.363112	7999.839830	14.250791	-0.051222	4.815517
243.361949	7999.899637	14.255795	-0.051222	4.815534
243.327809	7999.583004	14.260800	-0.051216	4.815442

243.325664	7996.367896	14.265805	-0.051213	4.814502
243.284404	7990.750090	14.270810	-0.051202	4.812859
243.314084	7983.966014	14.275815	-0.051204	4.810874
242.922653	7976.657696	14.280819	-0.051126	4.808737
243.069748	7969.037116	14.285824	-0.051149	4.806504
243.155572	7961.219861	14.290829	-0.051160	4.804214
242.972029	7953.378794	14.295834	-0.051121	4.801916
242.874835	7945.395970	14.300839	-0.051098	4.799576
243.062911	7937.413857	14.305843	-0.051128	4.797233
242.984947	7929.408304	14.310848	-0.051108	4.794883
242.910117	7921.420574	14.315853	-0.051090	4.792538
242.921995	7913.375350	14.320858	-0.051087	4.790174
243.072422	7905.453897	14.325863	-0.051110	4.787844
242.711401	7897.361506	14.330867	-0.051038	4.785466
242.798007	7889.425760	14.335872	-0.051049	4.783130
242.606065	7881.416972	14.340877	-0.051008	4.780773
242.798680	7873.418367	14.345882	-0.051039	4.778416
242.514485	7865.404711	14.350887	-0.050981	4.776056
242.519282	7857.384029	14.355891	-0.050977	4.773691
242.631654	7849.391967	14.360896	-0.050993	4.771333
242.580122	7841.379570	14.365901	-0.050979	4.768968
242.417508	7833.389894	14.370906	-0.050943	4.766609
242.394240	7825.371062	14.375911	-0.050934	4.764240
242.348320	7817.424604	14.380915	-0.050921	4.761892
242.356743	7809.363464	14.385920	-0.050917	4.759508
242.468015	7801.416205	14.390925	-0.050933	4.757156
242.272887	7793.359722	14.395930	-0.050892	4.754772
242.094977	7785.353924	14.400935	-0.050854	4.752401
242.066423	7777.288522	14.405939	-0.050843	4.750011
242.102985	7769.346860	14.410944	-0.050845	4.747657
241.984409	7761.327527	14.415949	-0.050818	4.745278
242.008300	7753.323206	14.420954	-0.050818	4.742903
242.285026	7745.380122	14.425959	-0.050864	4.740544
242.133846	7737.320011	14.430963	-0.050831	4.738150
242.035549	7729.352768	14.435968	-0.050808	4.735782
242.083701	7721.355269	14.440973	-0.050812	4.733404
241.971279	7713.292084	14.445978	-0.050786	4.731005
241.819826	7705.287206	14.450983	-0.050753	4.728622
241.844473	7697.328883	14.455987	-0.050752	4.726252
241.798516	7689.280703	14.460992	-0.050739	4.723854
241.823376	7681.358692	14.465997	-0.050738	4.721492
241.802460	7673.251901	14.471002	-0.050730	4.719074
241.740763	7665.366492	14.476007	-0.050713	4.716721
241.618728	7657.295355	14.481011	-0.050685	4.714312
241.473710	7649.323299	14.486016	-0.050654	4.711931
241.546496	7641.264055	14.491021	-0.050662	4.709522
241.518802	7633.282274	14.496026	-0.050652	4.707135
241.549107	7625.309154	14.501031	-0.050653	4.704749
241.478402	7617.295568	14.506035	-0.050635	4.702351
241.549997	7609.344401	14.511040	-0.050643	4.699969
241.357945	7601.329866	14.516045	-0.050602	4.697568
241.228342	7593.294928	14.521050	-0.050573	4.695160
241.367522	7585.315803	14.526055	-0.050594	4.692766
241.294378	7577.228132	14.531059	-0.050575	4.690339
241.256176	7569.307048	14.536064	-0.050563	4.687961
241.167330	7561.281666	14.541069	-0.050542	4.685550
241.419824	7553.293486	14.546074	-0.050584	4.683148
241.378388	7545.330589	14.551079	-0.050571	4.680754
240.934464	7537.294008	14.556083	-0.050484	4.678336
240.933160	7529.332365	14.561088	-0.050479	4.675940
240.987629	7521.251758	14.566093	-0.050484	4.673506
240.722702	7513.114868	14.571098	-0.050429	4.671054
240.887837	7505.220244	14.576103	-0.050455	4.668673
240.882465	7497.230592	14.581107	-0.050449	4.666263
240.772394	7489.199165	14.586112	-0.050424	4.663839
240.717782	7481.273463	14.591117	-0.050409	4.661446
240.798833	7473.218046	14.596122	-0.050419	4.659012
240.646598	7465.279606	14.601127	-0.050385	4.656613
240.650248	7457.227143	14.606131	-0.050381	4.654177
240.812497	7449.221661	14.611136	-0.050406	4.651754
240.914519	7441.214974	14.616141	-0.050420	4.649330
240.617846	7433.218611	14.621146	-0.050360	4.646908
240.502808	7425.176514	14.626151	-0.050334	4.644471
240.637684	7417.237022	14.631155	-0.050354	4.642063
240.350741	7409.170110	14.636160	-0.050296	4.639616
240.433408	7401.289204	14.641165	-0.050306	4.637223
240.234538	7393.186828	14.646170	-0.050264	4.634763
240.364068	7385.217697	14.651175	-0.050283	4.632341
240.155222	7377.173229	14.656179	-0.050239	4.629895
240.021251	7369.181401	14.661184	-0.050209	4.627464
240.073753	7361.183735	14.666189	-0.050214	4.625030
240.027758	7353.213777	14.671194	-0.050201	4.622603
240.288229	7345.191829	14.676199	-0.050244	4.620158
240.261901	7337.179076	14.681203	-0.050234	4.617716
240.068810	7329.176710	14.686208	-0.050194	4.615275
240.217202	7321.192936	14.691213	-0.050216	4.612839
240.085983	7313.140842	14.696218	-0.050187	4.610380
240.133864	7305.213568	14.701223	-0.050191	4.607958
240.092425	7297.161850	14.706227	-0.050178	4.605497
240.193613	7289.176589	14.711232	-0.050192	4.603055
240.043826	7281.189686	14.716237	-0.050159	4.600611
239.848597	7273.184724	14.721242	-0.050118	4.598161
239.870589	7265.206208	14.726247	-0.050117	4.595717
239.802686	7257.155706	14.731251	-0.050099	4.593249
239.531425	7249.106890	14.736256	-0.050044	4.590781
239.473759	7241.140408	14.741261	-0.050028	4.588337
239.374213	7233.095939	14.746266	-0.050005	4.585867
239.670080	7225.170729	14.751271	-0.050055	4.583433
239.579654	7217.110480	14.756275	-0.050033	4.580956
239.327391	7209.097728	14.761280	-0.049981	4.578493
239.364054	7201.127073	14.766285	-0.049983	4.576041
239.332364	7193.119330	14.771290	-0.049972	4.573576
239.287631	7185.117995	14.776295	-0.049959	4.571112
239.331056	7177.101436	14.781299	-0.049962	4.568641
239.271270	7169.127054	14.786304	-0.049946	4.566183
239.188787	7161.155065	14.791309	-0.049926	4.563724
239.058167	7153.156265	14.796314	-0.049896	4.561255
239.096918	7145.142918	14.801319	-0.049898	4.558780
238.963996	7137.173088	14.806323	-0.049869	4.556318
238.958935	7129.117160	14.811328	-0.049863	4.553827
239.027441	7121.127846	14.816333	-0.049871	4.551356
238.928639	7113.057991	14.821338	-0.049847	4.548859
238.804108	7105.115724	14.826343	-0.049819	4.546399
238.752737	7097.094797	14.831347	-0.049805	4.543914
238.789349	7089.131144	14.836352	-0.049807	4.541445
238.769150	7081.118817	14.841357	-0.049798	4.538960
238.649317	7073.166822	14.846362	-0.049771	4.536492
238.711490	7065.145682	14.851367	-0.049777	4.534002
238.630744	7057.096711	14.856371	-0.049757	4.531501
238.508648	7049.117767	14.861376	-0.049729	4.529021
238.550728	7041.141112	14.866381	-0.049732	4.526540
238.647225	7033.111264	14.871386	-0.049745	4.524041
238.550572	7025.168428	14.876391	-0.049722	4.521568
238.394067	7017.095177	14.881395	-0.049688	4.519053
238.336358	7009.140883	14.886400	-0.049673	4.516573
238.427388	7001.078732	14.891405	-0.049685	4.514059
238.324130	6992.994606	14.896410	-0.049660	4.511536
238.240832	6985.030845	14.901415	-0.049640	4.509050
238.074718	6977.053234	14.906419	-0.049604	4.506557
237.978213	6969.015602	14.911424	-0.049581	4.504044
238.238006	6961.105095	14.916429	-0.049625	4.501571
238.181763	6953.054078	14.921434	-0.049609	4.499052
238.159529	6945.128904	14.926439	-0.049600	4.496570
238.125836	6937.064760	14.931443	-0.049589	4.494044
238.248722	6929.040509	14.936448	-0.049607	4.491529
238.239787	6921.065793	14.941453	-0.049600	4.489028
238.032503	6913.046789	14.946458	-0.049556	4.486511
238.082338	6905.047647	14.951463	-0.049561	4.484000
237.871159	6897.078536	14.956467	-0.049517	4.481496
237.825674	6889.052640	14.961472	-0.049503	4.478973
237.660940	6881.062348	14.966477	-0.049467	4.476459
237.711250	6873.062356	14.971482	-0.049472	4.473942
237.729708	6865.053331	14.976487	-0.049470	4.471420
237.717846	6857.009541	14.981491	-0.049463	4.468886
237.710246	6849.012853	14.986496	-0.049457	4.466366
237.433685	6841.063433	14.991501	-0.049400	4.463857
237.472914	6833.025815	14.996506	-0.049403	4.461321
237.504877	6825.058086	15.001511	-0.049404	4.458805
237.577854	6817.034082	15.006515	-0.049412	4.456271
237.428479	6809.019380	15.011520	-0.049380	4.453736
237.351863	6800.995553	15.016525	-0.049360	4.451198
237.314790	6792.968927	15.021530	-0.049348	4.448658
237.409953	6785.013186	15.026535	-0.049361	4.446139
237.206302	6777.011716	15.031539	-0.049318	4.443603
237.181919	6769.042019	15.036544	-0.049309	4.441076
237.174478	6761.037285	15.041549	-0.049302	4.438537
237.092177	6753.028346	15.046554	-0.049282	4.435995
237.171285	6744.966730	15.051559	-0.049292	4.433435
237.260597	6736.916477	15.056563	-0.049304	4.430878
237.155021	6728.940416	15.061568	-0.049279	4.428341
237.088469	6720.975271	15.066573	-0.049262	4.425807
237.072698	6712.962978	15.071578	-0.049254	4.423257
237.062220	6704.987580	15.076583	-0.049247	4.420717
236.927701	6696.987325	15.081587	-0.049217	4.418167
236.797042	6688.984839	15.086592	-0.049188	4.415615
236.889337	6680.995296	15.091597	-0.049200	4.413066
236.856280	6672.951703	15.096602	-0.049189	4.410498
236.957306	6665.020110	15.101607	-0.049203	4.407965
236.760700	6656.959188	15.106611	-0.049161	4.405388
236.744564	6648.953792	15.111616	-0.049153	4.402828
236.906596	6640.972547	15.116621	-0.049178	4.400275
236.832954	6633.004705	15.121626	-0.049160	4.397724
236.746173	6625.018363	15.126631	-0.049138	4.395165
236.547116	6616.984112	15.131635	-0.049096	4.392589
236.573180	6608.912800	15.136640	-0.049096	4.390000
236.479604	6600.973809	15.141645	-0.049074	4.387452
236.537153	6592.919179	15.146650	-0.049080	4.384866
236.609510	6585.027366	15.151655	-0.049088	4.382331
236.539761	6576.965002	15.156659	-0.049070	4.379739
236.332145	6569.010886	15.161664	-0.049027	4.377179
236.235423	6561.012912	15.166669	-0.049004	4.374605
236.227163	6552.957948	15.171674	-0.048997	4.372010
236.247433	6544.940169	15.176679	-0.048996	4.369427
236.095887	6536.976877	15.181683	-0.048963	4.366859
235.968329	6528.971439	15.186688	-0.048934	4.364275
236.201393	6521.047888	15.191693	-0.048973	4.361719
236.156521	6512.944008	15.196698	-0.048959	4.359101
236.048520	6505.047143	15.201703	-0.048934	4.356548
236.010893	6496.939285	15.206707	-0.048922	4.353926
235.926845	6488.868140	15.211712	-0.048902	4.351314
235.965732	6480.853350	15.216717	-0.048904	4.348719
235.826504	6472.896147	15.221722	-0.048873	4.346140
235.804888	6464.989420	15.226727	-0.048864	4.343577
235.591486	6456.944186	15.231731	-0.048819	4.340966
235.811079	6448.932196	15.236736	-0.048855	4.338367
235.660452	6440.976108	15.241741	-0.048822	4.335783
235.569598	6432.933252	15.246746	-0.048800	4.333169
235.494882	6424.935258	15.251751	-0.048781	4.330568
235.486627	6416.938725	15.256755	-0.048775	4.327966
235.439176	6408.935417	15.261760	-0.048761	4.325361
235.382869	6400.969735	15.266765	-0.048746	4.322766
235.402574	6392.956395	15.271770	-0.048744	4.320154
235.423464	6384.986155	15.276775	-0.048743	4.317555
235.090860	6376.940841	15.281779	-0.048676	4.314927
235.234595	6368.947840	15.286784	-0.048698	4.312318
235.174629	6360.897515	15.291789	-0.048682	4.309688
235.026842	6352.885711	15.296794	-0.048650	4.307067
235.142536	6344.925068	15.301799	-0.048666	4.304464
234.902213	6336.936724	15.306803	-0.048617	4.301848
235.017051	6328.891405	15.311808	-0.048633	4.299214
235.029255	6320.947760	15.316813	-0.048630	4.296611
235.155308	6312.871937	15.321818	-0.048649	4.293964
235.135452	6304.911192	15.326823	-0.048640	4.291351
234.992375	6296.886132	15.331827	-0.048609	4.288715
234.959600	6288.896552	15.336832	-0.048597	4.286090
234.972495	6280.897440	15.341837	-0.048595	4.283461
234.692258	6272.958158	15.346842	-0.048538	4.280847
234.937536	6264.950604	15.351847	-0.048579	4.278214
234.788337	6256.938196	15.356851	-0.048546	4.275574
234.697437	6248.893294	15.361856	-0.048524	4.272922
234.639323	6240.875286	15.366861	-0.048508	4.270278
234.565369	6232.876883	15.371866	-0.048489	4.267638
234.718545	6224.866068	15.376871	-0.048513	4.264995
234.547786	6216.883033	15.381875	-0.048476	4.262356
234.419001	6208.876502	15.386880	-0.048447	4.259708
234.554025	6200.931987	15.391885	-0.048467	4.257082
234.401214	6192.858773	15.396890	-0.048434	4.254408
234.455191	6184.903734	15.401895	-0.048439	4.251774
234.384964	6176.888311	15.406899	-0.048421	4.249118
234.266617	6168.915994	15.411904	-0.048394	4.246473
234.305551	6160.895349	15.416909	-0.048396	4.243812
234.274192	6152.912743	15.421914	-0.048386	4.241161
234.380164	6144.952829	15.426919	-0.048400	4.238518
234.101434	6136.942258	15.431923	-0.048344	4.235852
233.883986	6128.907865	15.436928	-0.048298	4.233178
234.258315	6120.900764	15.441933	-0.048363	4.230516
233.933463	6112.908781	15.446938	-0.048297	4.227851
233.789659	6104.926926	15.451943	-0.048266	4.225190
233.957400	6096.901589	15.456947	-0.048292	4.222515
234.000622	6088.905581	15.461952	-0.048295	4.219847
233.828100	6080.947294	15.466957	-0.048258	4.217188
233.699705	6072.926442	15.471962	-0.048229	4.214507
233.666082	6064.947069	15.476967	-0.048218	4.211839
233.693473	6056.900929	15.481971	-0.048218	4.209148
233.360151	6048.941007	15.486976	-0.048151	4.206480
233.463781	6040.924235	15.491981	-0.048165	4.203795
233.377979	6032.950137	15.496986	-0.048144	4.201122
233.524608	6024.923588	15.501991	-0.048167	4.198431
233.430303	6016.938595	15.506995	-0.048144	4.195750
233.418816	6008.839943	15.512000	-0.048137	4.193030
233.346059	6000.806104	15.517005	-0.048118	4.190330
233.253865	5992.824516	15.522010	-0.048096	4.187645
233.359964	5984.865769	15.527015	-0.048111	4.184968
233.348233	5976.903877	15.532019	-0.048104	4.182287
233.295524	5968.891013	15.537024	-0.048089	4.179587
233.465540	5960.941726	15.542029	-0.048116	4.176909
233.227866	5952.892604	15.547034	-0.048067	4.174191
233.315192	5944.893438	15.552039	-0.048078	4.171492
233.111827	5936.847290	15.557043	-0.048035	4.168772
233.080394	5928.856071	15.562048	-0.048024	4.166070
232.983303	5920.903661	15.567053	-0.048001	4.163379
232.989619	5912.860688	15.572058	-0.047998	4.160657
233.087072	5904.947021	15.577063	-0.048011	4.157978
232.670373	5896.916222	15.582067	-0.047928	4.155252
232.678519	5888.866892	15.587072	-0.047925	4.152522
232.926838	5880.843888	15.592077	-0.047966	4.149803
232.841122	5872.852503	15.597082	-0.047945	4.147088
232.697883	5864.836279	15.602087	-0.047914	4.144362
232.565792	5856.898430	15.607091	-0.047884	4.141662
232.485213	5848.884173	15.612096	-0.047864	4.138934
232.662787	5840.923711	15.617101	-0.047892	4.136226
232.357672	5832.846595	15.622106	-0.047830	4.133471
232.466384	5824.859748	15.627111	-0.047846	4.130749
232.317912	5816.849097	15.632115	-0.047813	4.128015
232.207932	5808.851552	15.637120	-0.047788	4.125283
232.280238	5800.922064	15.642125	-0.047796	4.122576
232.243570	5792.869414	15.647130	-0.047784	4.119823
232.356211	5784.935217	15.652135	-0.047800	4.117110
232.095500	5776.896197	15.657139	-0.047747	4.114355
232.350040	5768.832322	15.662144	-0.047789	4.111597
232.249016	5760.828209	15.667149	-0.047765	4.108852
232.159541	5752.855442	15.672154	-0.047744	4.106117
232.360813	5744.875997	15.677159	-0.047776	4.103381
232.028410	5736.870521	15.682163	-0.047710	4.100627
231.972432	5728.893485	15.687168	-0.047694	4.097885
232.089991	5720.931412	15.692173	-0.047711	4.095149
232.048327	5712.876536	15.697178	-0.047698	4.092376
231.815023	5704.896292	15.702183	-0.047650	4.089625
231.764765	5696.894379	15.707187	-0.047636	4.086867
231.712384	5688.869920	15.712192	-0.047621	4.084100
231.768267	5680.954254	15.717197	-0.047626	4.081369
231.449341	5672.945878	15.722202	-0.047562	4.078600
231.498968	5664.946330	15.727207	-0.047566	4.075836
231.617008	5656.914225	15.732211	-0.047583	4.073061
231.553023	5648.844428	15.737216	-0.047567	4.070268
231.696053	5640.835761	15.742221	-0.047588	4.067497
231.743796	5632.880543	15.747226	-0.047592	4.064742
231.731495	5624.939479	15.752231	-0.047585	4.061988
231.597023	5616.948592	15.757235	-0.047555	4.059214
231.705514	5608.957630	15.762240	-0.047570	4.056442
231.663612	5600.940640	15.767245	-0.047557	4.053656
231.538180	5592.874338	15.772250	-0.047529	4.050850
231.540317	5584.940183	15.777255	-0.047525	4.048090
231.490421	5576.916826	15.782259	-0.047510	4.045296
231.470026	5568.938099	15.787264	-0.047502	4.042516
231.298657	5560.927458	15.792269	-0.047465	4.039721
231.496131	5552.932556	15.797274	-0.047496	4.036935
231.211985	5544.964752	15.802279	-0.047439	4.034149
231.041663	5536.804679	15.807283	-0.047402	4.031296
231.034737	5528.839758	15.812288	-0.047396	4.028511
231.149390	5520.847386	15.817293	-0.047412	4.025717
231.204929	5512.857766	15.822298	-0.047417	4.022921
231.186280	5504.911700	15.827303	-0.047409	4.020137
230.985674	5496.923119	15.832307	-0.047367	4.017333
230.943403	5488.877118	15.837312	-0.047354	4.014510
230.801984	5480.887458	15.842317	-0.047323	4.011703
230.782733	5472.881098	15.847322	-0.047314	4.008890
230.853782	5464.906488	15.852327	-0.047322	4.006088
230.640755	5456.926332	15.857331	-0.047278	4.003277
230.797102	5448.937757	15.862336	-0.047302	4.000467
230.764575	5440.929688	15.867341	-0.047291	3.997646
230.471136	5432.892328	15.872346	-0.047231	3.994808
230.497395	5424.885025	15.877351	-0.047231	3.991983
230.746772	5416.851860	15.882355	-0.047273	3.989151
230.631135	5408.883638	15.887360	-0.047246	3.986334
230.397094	5400.874538	15.892365	-0.047198	3.983499
230.253471	5392.915532	15.897370	-0.047166	3.980681
230.392515	5384.960410	15.902375	-0.047187	3.977866
230.200009	5376.948107	15.907379	-0.047146	3.975024
230.189231	5368.916291	15.912384	-0.047139	3.972176
230.257443	5360.913758	15.917389	-0.047147	3.969338
230.064902	5352.971566	15.922394	-0.047106	3.966515
230.042272	5344.927720	15.927399	-0.047097	3.963657
230.071625	5336.949506	15.932403	-0.047097	3.960820
229.971975	5328.979728	15.937408	-0.047074	3.957983
229.839879	5321.005893	15.942413	-0.047044	3.955141
230.068943	5312.885385	15.947418	-0.047082	3.952251
229.960667	5304.894869	15.952423	-0.047057	3.949400
229.747331	5296.943319	15.957427	-0.047012	3.946559
229.811917	5288.966414	15.962432	-0.047019	3.943711
230.073287	5280.964552	15.967437	-0.047063	3.940856
229.809081	5272.950866	15.972442	-0.047009	3.937985
229.796251	5264.989027	15.977447	-0.047002	3.935135
229.804477	5256.931707	15.982451	-0.046998	3.932250
229.607536	5248.936765	15.987456	-0.046956	3.929381
229.713103	5240.995134	15.992461	-0.046971	3.926534
229.379736	5232.965820	15.997466	-0.046904	3.923646
229.386335	5224.984359	16.002471	-0.046900	3.920779
229.454992	5216.996891	16.007475	-0.046908	3.917909
229.446745	5208.945453	16.012480	-0.046902	3.915012
229.566260	5200.941093	16.017485	-0.046919	3.912133
229.288287	5192.916322	16.022490	-0.046862	3.909237
229.238798	5184.971478	16.027495	-0.046848	3.906371
229.321337	5176.962482	16.032499	-0.046859	3.903483
229.431997	5168.957918	16.037504	-0.046874	3.900595
229.383368	5161.021998	16.042509	-0.046860	3.897726
229.301627	5152.950425	16.047514	-0.046840	3.894806
229.103672	5144.975594	16.052519	-0.046798	3.891916
228.928073	5136.983187	16.057523	-0.046761	3.889019
228.817938	5128.992477	16.062528	-0.046735	3.886120
228.919364	5120.968958	16.067533	-0.046749	3.883212
228.905337	5112.952437	16.072538	-0.046741	3.880302
228.976241	5104.996658	16.077543	-0.046750	3.877414
228.761417	5096.990940	16.082547	-0.046705	3.874499
228.774124	5088.746548	16.087552	-0.046702	3.871500
228.784624	5080.840398	16.092557	-0.046699	3.868622
228.572231	5072.881191	16.097562	-0.046655	3.865718
228.898095	5064.903747	16.102567	-0.046710	3.862816
228.631269	5056.950169	16.107571	-0.046656	3.859908
228.743067	5048.972441	16.112576	-0.046672	3.856997
228.623375	5040.950299	16.117581	-0.046644	3.854063
228.465655	5032.932168	16.122586	-0.046610	3.851128
228.538247	5024.973056	16.127591	-0.046619	3.848216
228.549321	5016.970554	16.132595	-0.046616	3.845285
228.409200	5009.006470	16.137600	-0.046585	3.842363
228.383726	5001.026749	16.142605	-0.046575	3.839435
228.148846	4993.040301	16.147610	-0.046526	3.836498
228.208329	4985.046798	16.152615	-0.046532	3.833563
228.151578	4976.976037	16.157619	-0.046517	3.830594
227.917440	4968.994618	16.162624	-0.046468	3.827652
227.998521	4960.998011	16.167629	-0.046478	3.824709
228.183939	4953.026944	16.172634	-0.046508	3.821775
228.082617	4945.018368	16.177639	-0.046484	3.818819
228.057625	4937.042913	16.182643	-0.046475	3.815875
228.105352	4929.047447	16.187648	-0.046478	3.812923
227.915324	4921.053424	16.192653	-0.046438	3.809963
227.721587	4913.078570	16.197658	-0.046397	3.807008
228.058061	4905.041007	16.202663	-0.046455	3.804040
227.936948	4897.095427	16.207667	-0.046427	3.801093
227.774957	4889.070116	16.212672	-0.046392	3.798113
227.736591	4881.098522	16.217677	-0.046380	3.795154
227.664195	4873.021760	16.222682	-0.046362	3.792152
227.487697	4865.061732	16.227687	-0.046324	3.789190
227.422247	4857.058595	16.232691	-0.046307	3.786211
227.374157	4849.050692	16.237696	-0.046293	3.783229
227.508290	4841.046548	16.242701	-0.046313	3.780249
227.226016	4833.082987	16.247706	-0.046255	3.777273
227.410394	4825.049924	16.252711	-0.046285	3.774280
227.371253	4817.075167	16.257715	-0.046272	3.771300
227.189113	4809.065349	16.262720	-0.046234	3.768302
227.158106	4801.064437	16.267725	-0.046223	3.765309
227.446780	4793.061150	16.272730	-0.046272	3.762319
227.224073	4785.069726	16.277735	-0.046225	3.759320
227.121672	4777.144774	16.282739	-0.046201	3.756346
227.008279	4769.082133	16.287744	-0.046175	3.753317
227.093209	4761.063601	16.292749	-0.046186	3.750308
226.775859	4753.076519	16.297754	-0.046122	3.747298
226.788298	4745.057982	16.302759	-0.046119	3.744282
226.811099	4737.133120	16.307763	-0.046119	3.741299
226.644569	4729.109691	16.312768	-0.046083	3.738272
226.609671	4721.112679	16.317773	-0.046071	3.735255
226.729696	4713.097469	16.322778	-0.046088	3.732233
226.666501	4705.093714	16.327783	-0.046072	3.729208
226.627940	4697.118034	16.332787	-0.046060	3.726193
226.719974	4689.113280	16.337792	-0.046072	3.723166
226.773051	4681.161176	16.342797	-0.046077	3.720157
226.465101	4673.167839	16.347802	-0.046014	3.717120
226.606883	4665.156334	16.352807	-0.046036	3.714086
226.578824	4657.069381	16.357811	-0.046026	3.711015
226.238440	4649.098913	16.362816	-0.045957	3.707979
226.208125	4641.117447	16.367821	-0.045947	3.704944
226.216336	4633.139210	16.372826	-0.045943	3.701908
226.200747	4625.179727	16.377831	-0.045936	3.698877
225.945566	4617.199908	16.382835	-0.045883	3.695829
226.178768	4609.161959	16.387840	-0.045922	3.692769
226.047044	4601.134200	16.392845	-0.045892	3.689701
225.715749	4593.186819	16.397850	-0.045825	3.686656
225.821362	4585.179640	16.402855	-0.045840	3.683597
225.907384	4577.193421	16.407859	-0.045851	3.680543
225.720937	4569.209162	16.412864	-0.045811	3.677480
225.866870	4561.246853	16.417869	-0.045834	3.674431
225.689887	4553.223288	16.422874	-0.045796	3.671348
225.741031	4545.187133	16.427879	-0.045800	3.668264
225.498928	4537.175885	16.432883	-0.045750	3.665178
225.636495	4529.193669	16.437888	-0.045771	3.662112
225.650934	4521.217523	16.442893	-0.045769	3.659041
225.397605	4513.247666	16.447898	-0.045717	3.655964
225.425163	4505.213673	16.452903	-0.045717	3.652867
225.290320	4497.216201	16.457907	-0.045687	3.649777
225.101383	4489.239783	16.462912	-0.045647	3.646691
225.021087	4481.271607	16.467917	-0.045627	3.643608
225.029887	4473.275031	16.472922	-0.045623	3.640514
225.145840	4465.277837	16.477927	-0.045640	3.637420
224.933846	4457.249780	16.482931	-0.045596	3.634303
224.868984	4449.220884	16.487936	-0.045579	3.631186
225.210481	4441.215559	16.492941	-0.045637	3.628087
225.006028	4433.210973	16.497946	-0.045594	3.624971
224.921156	4425.277988	16.502951	-0.045573	3.621884
224.905614	4417.274780	16.507955	-0.045566	3.618768
225.023463	4409.267461	16.512960	-0.045583	3.615652
224.878269	4401.278411	16.517965	-0.045551	3.612532
224.736374	4393.244922	16.522970	-0.045519	3.609393
224.885001	4385.291291	16.527975	-0.045542	3.606291
224.676039	4377.332440	16.532979	-0.045498	3.603173
224.662460	4369.329912	16.537984	-0.045491	3.600042
224.537340	4361.376623	16.542989	-0.045462	3.596923
224.507693	4353.339035	16.547994	-0.045452	3.593772
224.418039	4345.320003	16.552999	-0.045430	3.590623
224.321759	4337.337934	16.558003	-0.045407	3.587486
224.351699	4329.289427	16.563008	-0.045408	3.584324
224.310818	4321.392789	16.568013	-0.045395	3.581217
224.289527	4313.377948	16.573018	-0.045386	3.578061
224.472121	4305.367964	16.578023	-0.045415	3.574910
224.312050	4297.385327	16.583027	-0.045381	3.571757
224.297085	4289.359628	16.588032	-0.045373	3.568588
224.289254	4281.383983	16.593037	-0.045367	3.565437
224.220236	4273.389931	16.598042	-0.045349	3.562274
224.074975	4265.427584	16.603047	-0.045317	3.559118
223.959139	4257.448916	16.608051	-0.045290	3.555954
224.105166	4249.309955	16.613056	-0.045312	3.552731
224.062407	4241.298558	16.618061	-0.045299	3.549550
223.899494	4233.341852	16.623066	-0.045264	3.546385
224.001081	4225.347368	16.628071	-0.045278	3.543210
223.981833	4217.377725	16.633075	-0.045270	3.540038
223.748036	4209.448653	16.638080	-0.045221	3.536873
223.954611	4201.405827	16.643085	-0.045255	3.533672
223.670316	4193.390977	16.648090	-0.045197	3.530466
223.555658	4185.405034	16.653095	-0.045170	3.527273
223.410548	4177.406840	16.658099	-0.045138	3.524071
223.624642	4169.454067	16.663104	-0.045173	3.520896
223.549995	4161.481391	16.668109	-0.045155	3.517701
223.358957	4153.454087	16.673114	-0.045114	3.514477
223.552778	4145.424846	16.678119	-0.045145	3.511262
223.516360	4137.420638	16.683123	-0.045133	3.508047
223.350051	4129.446258	16.688128	-0.045098	3.504836
223.414956	4121.505551	16.693133	-0.045105	3.501644
223.314183	4113.489620	16.698138	-0.045081	3.498413
223.057514	4105.538197	16.703143	-0.045028	3.495200
223.014036	4097.530370	16.708147	-0.045015	3.491968
223.127377	4089.486016	16.713152	-0.045031	3.488723
223.299723	4081.514727	16.718157	-0.045058	3.485507
223.078369	4073.548533	16.723162	-0.045012	3.482277
223.052705	4065.570545	16.728167	-0.045003	3.479046
222.726384	4057.631460	16.733171	-0.044937	3.475818
222.676743	4049.550285	16.738176	-0.044923	3.472538
222.828311	4041.549926	16.743181	-0.044946	3.469294
222.649914	4033.541043	16.748186	-0.044908	3.466033
222.679956	4025.560723	16.753191	-0.044908	3.462788
222.521258	4017.589957	16.758195	-0.044874	3.459537
222.538332	4009.579736	16.763200	-0.044872	3.456272
222.701421	4001.573750	16.768205	-0.044897	3.453011
222.287003	3993.579789	16.773210	-0.044815	3.449733
222.437157	3985.616701	16.778215	-0.044838	3.446483
222.459171	3977.609663	16.783219	-0.044838	3.443208
222.242625	3969.639516	16.788224	-0.044792	3.439937
222.205943	3961.680684	16.793229	-0.044781	3.436673
222.341481	3953.619558	16.798234	-0.044801	3.433370
222.323190	3945.615941	16.803239	-0.044792	3.430082
222.000482	3937.662423	16.808243	-0.044727	3.426802
221.856443	3929.650430	16.813248	-0.044696	3.423500
222.136759	3921.669619	16.818253	-0.044743	3.420222
221.959383	3913.690978	16.823258	-0.044705	3.416926
222.068447	3905.708517	16.828263	-0.044720	3.413636
221.988243	3897.661779	16.833267	-0.044700	3.410309
221.898222	3889.687897	16.838272	-0.044679	3.407009
221.893521	3881.708645	16.843277	-0.044673	3.403706
221.943562	3873.718262	16.848282	-0.044677	3.400397
221.916618	3865.754121	16.853287	-0.044667	3.397094
221.725714	3857.733325	16.858291	-0.044627	3.393757
221.776125	3849.652151	16.863296	-0.044631	3.390401
221.977021	3841.682559	16.868301	-0.044664	3.387093
221.690455	3833.710133	16.873306	-0.044605	3.383764
221.673372	3825.758062	16.878311	-0.044597	3.380450
221.643421	3817.792455	16.883315	-0.044587	3.377126
221.518447	3809.789735	16.888320	-0.044558	3.373779
221.493802	3801.790195	16.893325	-0.044549	3.370435
221.503189	3793.775568	16.898330	-0.044546	3.367082
221.562681	3785.816785	16.903335	-0.044552	3.363751
221.394240	3777.845235	16.908339	-0.044515	3.360403
221.399922	3769.848887	16.913344	-0.044512	3.357047
221.324673	3761.845973	16.918349	-0.044493	3.353682
221.223482	3753.799942	16.923354	-0.044469	3.350295
221.230046	3745.843207	16.928359	-0.044465	3.346946
221.086639	3737.860059	16.933363	-0.044433	3.343577
221.035968	3729.856245	16.938368	-0.044419	3.340200
221.003185	3721.906296	16.943373	-0.044408	3.336842
220.754830	3713.892393	16.948378	-0.044357	3.333446
220.808858	3705.885372	16.953383	-0.044362	3.330060
220.593138	3697.933728	16.958387	-0.044317	3.326685
220.763033	3689.914383	16.963392	-0.044343	3.323292
220.705847	3681.930524	16.968397	-0.044328	3.319901
220.600334	3673.966467	16.973402	-0.044303	3.316514
220.710942	3665.932024	16.978407	-0.044319	3.313102
220.527972	3657.927464	16.983411	-0.044280	3.309688
220.578635	3649.946359	16.988416	-0.044284	3.306289
220.601002	3641.965721	16.993421	-0.044284	3.302886
220.518761	3633.977067	16.998426	-0.044263	3.299471
220.503750	3626.016988	17.003431	-0.044256	3.296068
220.360358	3618.021962	17.008435	-0.044224	3.292642
220.387173	3609.975591	17.013440	-0.044224	3.289197
220.275232	3602.036742	17.018445	-0.044198	3.285788
220.244017	3594.042922	17.023450	-0.044187	3.282356
220.148488	3586.078552	17.028455	-0.044165	3.278930
220.145613	3578.086586	17.033459	-0.044159	3.275492
220.167375	3570.061642	17.038464	-0.044158	3.272038
220.174348	3562.085605	17.043469	-0.044155	3.268600
220.145518	3554.069159	17.048474	-0.044144	3.265140
220.147927	3546.094490	17.053479	-0.044140	3.261696
219.998336	3538.119084	17.058483	-0.044107	3.258241
219.777663	3530.115488	17.063488	-0.044061	3.254768
219.949006	3522.093832	17.068493	-0.044088	3.251299
219.708358	3514.108580	17.073498	-0.044038	3.247825
219.638509	3506.134888	17.078503	-0.044020	3.244360
219.847705	3498.181955	17.083507	-0.044054	3.240911
219.760327	3490.193926	17.088512	-0.044033	3.237431
219.732564	3482.201825	17.093517	-0.044023	3.233948
219.635576	3474.107468	17.098522	-0.044000	3.230414
219.719926	3466.135155	17.103527	-0.044011	3.226937
219.439132	3458.182720	17.108531	-0.043953	3.223450
219.316893	3450.222023	17.113536	-0.043926	3.219961
219.365870	3442.251080	17.118541	-0.043930	3.216472
219.190461	3434.219522	17.123546	-0.043892	3.212943
219.147101	3426.214983	17.128551	-0.043879	3.209427
219.211103	3418.255239	17.133555	-0.043886	3.205932
219.327952	3410.271482	17.138560	-0.043903	3.202424
219.167337	3402.331965	17.143565	-0.043868	3.198921
219.135079	3394.306928	17.148570	-0.043857	3.195381
219.119150	3386.309746	17.153575	-0.043849	3.191850
219.258394	3378.297425	17.158579	-0.043870	3.188316
219.131508	3370.286946	17.163584	-0.043842	3.184766
219.207665	3362.357581	17.168589	-0.043851	3.181258
218.875332	3354.399467	17.173594	-0.043784	3.177715
218.836645	3346.384867	17.178599	-0.043772	3.174156
219.019500	3338.367737	17.183603	-0.043801	3.170602
218.938487	3330.372391	17.188608	-0.043781	3.167041
218.780407	3322.404751	17.193613	-0.043747	3.163486
218.782189	3314.399844	17.198618	-0.043742	3.159917
218.600958	3306.467214	17.203623	-0.043703	3.156368
218.611941	3298.460634	17.208627	-0.043700	3.152791
218.554457	3290.419609	17.213632	-0.043685	3.149191
218.459004	3282.463275	17.218637	-0.043662	3.145623
218.328179	3274.470777	17.223642	-0.043633	3.142033
218.464181	3266.486297	17.228647	-0.043653	3.138455
218.455793	3258.490354	17.233651	-0.043646	3.134861
218.412638	3250.502161	17.238656	-0.043633	3.131264
218.466703	3242.537115	17.243661	-0.043639	3.127679
218.215109	3234.535327	17.248666	-0.043587	3.124059
218.224291	3226.579275	17.253671	-0.043584	3.120467
218.265804	3218.607772	17.258675	-0.043586	3.116865
218.097867	3210.611849	17.263680	-0.043550	3.113239
218.229863	3202.611938	17.268685	-0.043570	3.109620
217.938580	3194.617493	17.273690	-0.043511	3.105981
217.943793	3186.635169	17.278695	-0.043507	3.102356
217.925407	3178.681010	17.283699	-0.043498	3.098738
218.011416	3170.661228	17.288704	-0.043509	3.095092
217.837408	3162.708535	17.293709	-0.043472	3.091459
217.621490	3154.686085	17.298714	-0.043427	3.087789
217.637847	3146.693513	17.303719	-0.043425	3.084138
217.557446	3138.755671	17.308723	-0.043405	3.080504
217.433585	3130.771690	17.313728	-0.043377	3.076842
217.463118	3122.734724	17.318733	-0.043378	3.073159
217.542250	3114.658825	17.323738	-0.043387	3.069455
217.364415	3106.713908	17.328743	-0.043349	3.065796
217.385364	3098.764345	17.333747	-0.043348	3.062139
217.557842	3090.762689	17.338752	-0.043375	3.058461
217.516030	3082.810156	17.343757	-0.043363	3.054791
217.254480	3074.823585	17.348762	-0.043309	3.051090
217.190273	3066.854849	17.353767	-0.043292	3.047403
217.095277	3058.880099	17.358771	-0.043269	3.043707
216.870948	3050.888069	17.363776	-0.043223	3.039992
217.001020	3042.936442	17.368781	-0.043242	3.036308
216.949630	3034.898402	17.373786	-0.043227	3.032571
216.766083	3026.916235	17.378791	-0.043188	3.028849
216.881988	3018.925504	17.383795	-0.043205	3.025133
216.858505	3010.945702	17.388800	-0.043196	3.021411
217.080533	3002.971457	17.393805	-0.043232	3.017698
216.813181	2995.003454	17.398810	-0.043177	3.013960
216.976783	2986.962914	17.403815	-0.043203	3.010205
216.912615	2979.012863	17.408819	-0.043186	3.006476
216.812311	2971.035292	17.413824	-0.043162	3.002728
216.530767	2963.110105	17.418829	-0.043105	2.998990
216.494210	2955.108022	17.423834	-0.043093	2.995224
216.401189	2947.108093	17.428839	-0.043071	2.991452
216.423770	2939.096115	17.433843	-0.043070	2.987674
216.361920	2931.090019	17.438848	-0.043054	2.983891
216.334168	2923.147231	17.443853	-0.043044	2.980134
216.082628	2915.190238	17.448858	-0.042992	2.976355
216.234884	2907.165438	17.453863	-0.043015	2.972559
216.333356	2899.162485	17.458867	-0.043029	2.968765
216.230025	2891.181510	17.463872	-0.043004	2.964967
216.214463	2883.244003	17.468877	-0.042997	2.961190
216.002256	2875.261842	17.473882	-0.042952	2.957376
216.082766	2867.285986	17.478887	-0.042962	2.953575
216.019920	2859.287511	17.483891	-0.042946	2.949751
215.968297	2851.278656	17.488896	-0.042931	2.945918
216.166433	2843.311803	17.493901	-0.042963	2.942113
215.671169	2835.355001	17.498906	-0.042866	2.938272
215.807764	2827.358302	17.503911	-0.042886	2.934439
215.989956	2819.343647	17.508915	-0.042915	2.930595
215.708889	2811.356949	17.513920	-0.042858	2.926736
215.559753	2803.431224	17.518925	-0.042825	2.922907
215.719234	2795.430433	17.523930	-0.042850	2.919054
215.607313	2787.463462	17.528935	-0.042824	2.915197
215.288153	2779.431900	17.533939	-0.042760	2.911293
215.423488	2771.406274	17.538944	-0.042780	2.907411
215.369802	2763.455231	17.543949	-0.042765	2.903550
215.158920	2755.513553	17.548954	-0.042721	2.899679
215.016422	2747.555140	17.553959	-0.042689	2.895799
215.064662	2739.547889	17.558963	-0.042693	2.891900
214.990135	2731.548427	17.563968	-0.042675	2.887994
214.957174	2723.574360	17.568973	-0.042664	2.884096
215.012042	2715.604484	17.573978	-0.042669	2.880200
215.109918	2707.629730	17.578983	-0.042682	2.876299
215.019410	2699.630220	17.583987	-0.042660	2.872370
214.838442	2691.644858	17.588992	-0.042622	2.868437
215.011988	2683.645322	17.593997	-0.042649	2.864512
214.725781	2675.719773	17.599002	-0.042591	2.860592
214.795149	2667.724063	17.604007	-0.042599	2.856652
214.907451	2659.729446	17.609011	-0.042615	2.852710
214.673375	2651.752813	17.614016	-0.042566	2.848752
214.422561	2643.812595	17.619021	-0.042515	2.844805
214.531920	2635.843299	17.624026	-0.042530	2.840858
214.589152	2627.871468	17.629031	-0.042536	2.836902
214.378810	2619.880342	17.634035	-0.042492	2.832915
214.324851	2611.857692	17.639040	-0.042477	2.828917
214.555384	2603.856451	17.644045	-0.042515	2.824939
214.375368	2595.928316	17.649050	-0.042476	2.820969
214.245991	2587.948878	17.654055	-0.042447	2.816970
214.297180	2579.966961	17.659059	-0.042452	2.812975
214.218998	2571.963965	17.664064	-0.042432	2.808956
214.121516	2564.010708	17.669069	-0.042409	2.804955
214.274030	2556.031945	17.674074	-0.042433	2.800950
214.157284	2548.081382	17.679079	-0.042406	2.796938
213.985614	2540.104126	17.684083	-0.042369	2.792903
213.846851	2532.088982	17.689088	-0.042338	2.788846
213.817465	2524.111718	17.694093	-0.042328	2.784808
213.591291	2516.167702	17.699098	-0.042281	2.780769
213.718830	2508.176303	17.704103	-0.042300	2.776721
213.657819	2500.207442	17.709107	-0.042283	2.772668
213.635604	2492.209564	17.714112	-0.042274	2.768596
213.500232	2484.258749	17.719117	-0.042244	2.764536
213.455233	2476.288308	17.724122	-0.042231	2.760465
213.741852	2468.280920	17.729127	-0.042279	2.756389
213.602139	2460.267749	17.734131	-0.042248	2.752278
213.478478	2452.256824	17.739136	-0.042220	2.748163
213.594835	2444.301314	17.744141	-0.042237	2.744085
213.503467	2436.330566	17.749146	-0.042215	2.739981
213.349502	2428.384676	17.754151	-0.042181	2.735879
213.436233	2420.390778	17.759155	-0.042192	2.731761
213.322328	2412.421856	17.764160	-0.042166	2.727638
213.213480	2404.482534	17.769165	-0.042141	2.723523
213.128820	2396.518668	17.774170	-0.042120	2.719392
213.131978	2388.554659	17.779175	-0.042116	2.715259
213.074151	2380.551842	17.784179	-0.042100	2.711096
213.043235	2372.555127	17.789184	-0.042090	2.706932
213.187824	2364.595149	17.794189	-0.042112	2.702791
212.932949	2356.647500	17.799194	-0.042059	2.698625
212.812385	2348.679989	17.804199	-0.042032	2.694451
212.749582	2340.691719	17.809203	-0.042015	2.690263
212.860860	2332.675271	17.814208	-0.042031	2.686065
213.029057	2324.729123	17.819213	-0.042057	2.681901
212.783229	2316.786688	17.824218	-0.042007	2.677706
212.814835	2308.801272	17.829223	-0.042008	2.673499
212.684233	2300.797295	17.834227	-0.041978	2.669266
212.453075	2292.840160	17.839232	-0.041930	2.665044
212.409741	2284.895837	17.844237	-0.041917	2.660834
212.302304	2276.927825	17.849242	-0.041892	2.656601
212.365944	2268.914065	17.854247	-0.041899	2.652348
212.404533	2260.954587	17.859251	-0.041902	2.648116
212.306681	2252.979773	17.864256	-0.041878	2.643859
212.211433	2245.024840	17.869261	-0.041856	2.639606
211.984248	2237.092599	17.874266	-0.041809	2.635350
212.126167	2229.057028	17.879271	-0.041830	2.631056
212.001899	2221.099918	17.884275	-0.041802	2.626780
211.678928	2213.154282	17.889280	-0.041737	2.622489
211.848474	2205.174454	17.894285	-0.041763	2.618206
211.912865	2197.178382	17.899290	-0.041771	2.613900
211.663384	2189.209308	17.904295	-0.041719	2.609580
211.640788	2181.253024	17.909299	-0.041710	2.605276
211.841759	2173.262170	17.914304	-0.041742	2.600960
211.893868	2165.324593	17.919309	-0.041747	2.596657
211.530039	2157.248407	17.924314	-0.041675	2.592242
211.743989	2149.179447	17.929319	-0.041709	2.587863
211.702746	2141.251525	17.934323	-0.041697	2.583537
211.489962	2133.336750	17.939328	-0.041652	2.579198
211.351604	2125.430327	17.944333	-0.041622	2.574862
211.308143	2117.439987	17.949338	-0.041609	2.570479
211.301706	2109.470270	17.954343	-0.041602	2.566103
210.973871	2101.559581	17.959347	-0.041536	2.561729
211.258507	2093.549700	17.964352	-0.041584	2.557335
211.355917	2085.595787	17.969357	-0.041598	2.552952
211.023133	2077.632220	17.974362	-0.041531	2.548526
210.912759	2069.664827	17.979367	-0.041505	2.544105
211.056151	2061.694775	17.984371	-0.041527	2.539694
210.994697	2053.740185	17.989376	-0.041511	2.535268
211.044167	2045.763219	17.994381	-0.041515	2.530831
210.910483	2037.801542	17.999386	-0.041485	2.526381
210.901706	2029.841596	18.004391	-0.041479	2.521933
210.932487	2021.912073	18.009395	-0.041479	2.517497
210.766302	2013.909989	18.014400	-0.041443	2.512998
210.801248	2005.928101	18.019405	-0.041445	2.508518
210.356311	1997.986256	18.024410	-0.041357	2.504016
210.275744	1990.028257	18.029415	-0.041337	2.499524
210.553321	1982.051849	18.034419	-0.041384	2.495040
210.504734	1974.051328	18.039424	-0.041370	2.490510
210.275744	1966.125918	18.044429	-0.041323	2.486002
210.237860	1958.158899	18.049434	-0.041311	2.481475
210.313567	1950.193035	18.054439	-0.041320	2.476949
210.381191	1942.231509	18.059443	-0.041327	2.472417
210.093028	1934.266190	18.064448	-0.041269	2.467848
210.345076	1926.285326	18.069453	-0.041311	2.463301
210.242389	1918.345014	18.074458	-0.041287	2.458743
210.120425	1910.388052	18.079463	-0.041259	2.454166
210.130080	1902.416540	18.084467	-0.041256	2.449581
209.894737	1894.465058	18.089472	-0.041207	2.444981
210.037792	1886.516446	18.094477	-0.041229	2.440403
210.034410	1878.549642	18.099482	-0.041223	2.435794
209.737471	1870.554303	18.104487	-0.041163	2.431138
209.751922	1862.574945	18.109491	-0.041161	2.426505
209.514809	1854.635249	18.114496	-0.041112	2.421868
209.507352	1846.694915	18.119501	-0.041105	2.417239
209.429060	1838.723113	18.124506	-0.041086	2.412577
209.457120	1830.740366	18.129511	-0.041086	2.407908
209.485423	1822.792725	18.134515	-0.041087	2.403251
209.400139	1814.850118	18.139520	-0.041066	2.398579
209.290987	1806.915355	18.144525	-0.041041	2.393900
209.283721	1798.913265	18.149530	-0.041034	2.389180
209.245641	1790.964623	18.154535	-0.041022	2.384480
209.194167	1783.025561	18.159539	-0.041008	2.379776
208.900358	1775.094011	18.164544	-0.040948	2.375047
209.176538	1767.074787	18.169549	-0.040995	2.370302
208.961772	1759.142502	18.174554	-0.040950	2.365560
208.862596	1751.209360	18.179559	-0.040926	2.360818
208.975370	1743.259685	18.184563	-0.040942	2.356073
208.709294	1735.293891	18.189568	-0.040888	2.351278
208.605590	1727.325901	18.194573	-0.040864	2.346485
208.544421	1719.368481	18.199578	-0.040847	2.341692
208.626680	1711.398335	18.204583	-0.040858	2.336893
208.498592	1703.458386	18.209587	-0.040829	2.332086
208.464501	1695.489114	18.214592	-0.040818	2.327258
208.767944	1687.510153	18.219597	-0.040869	2.322443
208.522494	1679.605809	18.224602	-0.040819	2.317617
208.389684	1671.656347	18.229607	-0.040789	2.312763
208.521624	1663.679733	18.234611	-0.040809	2.307904
208.496999	1655.715541	18.239616	-0.040799	2.303030
208.463437	1647.786229	18.244621	-0.040788	2.298166
208.257542	1639.852996	18.249626	-0.040745	2.293274
208.028068	1631.901314	18.254631	-0.040697	2.288359
208.058964	1623.950160	18.259635	-0.040698	2.283456
207.902408	1616.014955	18.264640	-0.040664	2.278536
207.928645	1608.055098	18.269645	-0.040664	2.273605
207.956689	1600.009537	18.274650	-0.040664	2.268611
207.740294	1592.097224	18.279655	-0.040619	2.263668
207.658354	1584.176160	18.284659	-0.040599	2.258720
207.601628	1576.210624	18.289664	-0.040583	2.253735
207.563306	1568.256190	18.294669	-0.040571	2.248748
207.640408	1560.292394	18.299674	-0.040580	2.243754
207.638957	1552.361688	18.304679	-0.040575	2.238763
207.410281	1544.462625	18.309683	-0.040528	2.233760
207.230541	1536.500801	18.314688	-0.040489	2.228711
207.344042	1528.537918	18.319693	-0.040506	2.223676
207.230040	1520.607728	18.324698	-0.040479	2.218630
207.165489	1512.662481	18.329703	-0.040462	2.213567
207.150161	1504.699182	18.334707	-0.040455	2.208486
207.156552	1496.746998	18.339712	-0.040451	2.203402
207.037222	1488.838436	18.344717	-0.040424	2.198322
206.788031	1480.910025	18.349722	-0.040373	2.193206
206.908666	1472.888841	18.354727	-0.040390	2.188053
207.029903	1464.942653	18.359731	-0.040408	2.182935
206.856499	1457.015602	18.364736	-0.040370	2.177791
206.912539	1449.081269	18.369741	-0.040376	2.172651
206.838162	1441.128805	18.374746	-0.040357	2.167475
206.779495	1433.208927	18.379751	-0.040341	2.162310
206.895082	1425.259977	18.384755	-0.040358	2.157129
206.643857	1417.332665	18.389760	-0.040306	2.151915
206.717904	1409.384600	18.394765	-0.040315	2.146706
206.515569	1401.463597	18.399770	-0.040273	2.141476
206.479489	1393.531367	18.404775	-0.040261	2.136241
206.303113	1385.611149	18.409779	-0.040223	2.130988
206.136291	1377.663561	18.414784	-0.040187	2.125705
206.386380	1369.707458	18.419789	-0.040229	2.120443
206.208322	1361.803863	18.424794	-0.040191	2.115162
206.066809	1353.796003	18.429799	-0.040159	2.109801
206.106415	1345.848990	18.434803	-0.040162	2.104485
206.018172	1337.924725	18.439808	-0.040141	2.099158
206.049058	1330.006356	18.444813	-0.040141	2.093833
205.820812	1322.070599	18.449818	-0.040094	2.088458
205.884746	1314.134151	18.454823	-0.040101	2.083097
205.894918	1306.209336	18.459827	-0.040098	2.077724
205.784987	1298.283969	18.464832	-0.040073	2.072326
205.720412	1290.349136	18.469837	-0.040056	2.066911
205.769976	1282.404981	18.474842	-0.040060	2.061487
205.877056	1274.472798	18.479847	-0.040075	2.056063
205.734643	1266.557383	18.484851	-0.040044	2.050611
205.509240	1258.640203	18.489856	-0.039997	2.045135
205.467952	1250.740125	18.494861	-0.039984	2.039674
205.454211	1242.821142	18.499866	-0.039977	2.034189
205.366610	1234.855591	18.504871	-0.039955	2.028648
205.213175	1226.934312	18.509875	-0.039922	2.023117
205.007256	1219.030487	18.514880	-0.039879	2.017577
205.013076	1211.088252	18.519885	-0.039875	2.012017
204.989466	1203.148541	18.524890	-0.039866	2.006440
204.957886	1195.225213	18.529895	-0.039855	2.000858
204.874392	1187.329050	18.534899	-0.039834	1.995275
204.599441	1179.409952	18.539904	-0.039778	1.989639
204.741864	1171.470025	18.544909	-0.039800	1.984017
204.556367	1163.569806	18.549914	-0.039760	1.978372
204.620842	1155.620903	18.554919	-0.039767	1.972703
204.903902	1147.656887	18.559923	-0.039815	1.967030
204.566133	1139.785239	18.564928	-0.039747	1.961340
204.519762	1131.888701	18.569933	-0.039734	1.955647
204.485968	1123.913163	18.574938	-0.039723	1.949882
204.384091	1115.995958	18.579943	-0.039699	1.944135
204.155797	1108.118651	18.584947	-0.039651	1.938385
204.026509	1100.195864	18.589952	-0.039622	1.932596
203.932135	1092.275424	18.594957	-0.039600	1.926796
204.146539	1084.327598	18.599962	-0.039635	1.920992
203.946362	1076.445044	18.604967	-0.039593	1.915172
203.968528	1068.525474	18.609971	-0.039592	1.909332
203.709654	1060.628011	18.614976	-0.039539	1.903459
203.754356	1052.729210	18.619981	-0.039542	1.897601
203.937829	1044.767505	18.624986	-0.039572	1.891693
203.723812	1036.879662	18.629991	-0.039527	1.885777
203.670512	1028.998069	18.634995	-0.039512	1.879866
203.617959	1021.097620	18.640000	-0.039497	1.873921
203.477775	1013.174239	18.645005	-0.039466	1.867931
203.365945	1005.270996	18.650010	-0.039441	1.861939
203.332856	997.371138	18.655015	-0.039430	1.855940
203.292287	989.460091	18.660019	-0.039417	1.849912
202.998691	981.587531	18.665024	-0.039358	1.843864
203.031220	973.690109	18.670029	-0.039359	1.837816
202.899139	965.797928	18.675034	-0.039329	1.831732
202.849972	957.877057	18.680039	-0.039315	1.825615
202.753163	950.001153	18.685043	-0.039292	1.819507
202.624905	942.106033	18.690048	-0.039264	1.813360
202.819294	934.161893	18.695053	-0.039295	1.807192
202.556958	926.302581	18.700058	-0.039241	1.801014
202.468947	918.424353	18.705063	-0.039220	1.794822
202.504944	910.460507	18.710067	-0.039222	1.788555
202.219106	902.586906	18.715072	-0.039164	1.782299
202.417842	894.680545	18.720077	-0.039196	1.776054
202.228881	886.800645	18.725082	-0.039156	1.769760
202.284680	878.905284	18.730087	-0.039161	1.763461
202.244459	871.037073	18.735091	-0.039149	1.757150
202.216721	863.135312	18.740096	-0.039139	1.750791
202.310957	855.238710	18.745101	-0.039151	1.744428
201.951097	847.417305	18.750106	-0.039079	1.738045
201.759290	839.542237	18.755111	-0.039039	1.731616
202.002187	831.619687	18.760115	-0.039079	1.725180
201.999076	823.747790	18.765120	-0.039074	1.718730
201.857347	815.891408	18.770125	-0.039043	1.712251
201.700287	808.006684	18.775130	-0.039008	1.705721
201.633692	800.139853	18.780135	-0.038991	1.699193
201.522910	792.281591	18.785139	-0.038966	1.692641
201.548797	784.373054	18.790144	-0.038966	1.686039
201.373982	776.538712	18.795149	-0.038928	1.679448
201.238089	768.684097	18.800154	-0.038898	1.672818
201.328694	760.769620	18.805159	-0.038910	1.666142
201.557642	752.884184	18.810163	-0.038948	1.659482
201.201044	745.070075	18.815168	-0.038876	1.652776
200.917486	737.237369	18.820173	-0.038819	1.646038
201.032390	729.360345	18.825178	-0.038835	1.639288
201.139166	721.458719	18.830183	-0.038850	1.632488
200.896106	713.593977	18.835187	-0.038800	1.625642
200.794859	705.747186	18.840192	-0.038776	1.618804
200.994614	697.860379	18.845197	-0.038809	1.611943
200.886157	690.007845	18.850202	-0.038784	1.605040
200.550598	682.226682	18.855207	-0.038716	1.598138
200.798560	674.328176	18.860211	-0.038758	1.591184
200.388948	666.533287	18.865216	-0.038677	1.584199
200.274294	658.706923	18.870221	-0.038650	1.577196
200.266538	650.841132	18.875226	-0.038644	1.570143
200.168744	643.014443	18.880231	-0.038621	1.563080
200.124089	635.192871	18.885235	-0.038608	1.555997
200.191799	627.304031	18.890240	-0.038616	1.548837
200.172373	619.471267	18.895245	-0.038607	1.541682
199.904208	611.679366	18.900250	-0.038552	1.534494
199.861889	603.826653	18.905255	-0.038540	1.527250
199.911462	595.999733	18.910259	-0.038544	1.520009
199.737960	588.194426	18.915264	-0.038507	1.512720
199.750799	580.357315	18.920269	-0.038504	1.505395
199.583040	572.569009	18.925274	-0.038468	1.498051
199.639832	564.722912	18.930279	-0.038474	1.490652
199.529629	556.931292	18.935283	-0.038449	1.483241
199.359638	549.140768	18.940288	-0.038412	1.475785
199.261948	541.284295	18.945293	-0.038389	1.468238
199.387136	533.444385	18.950298	-0.038408	1.460705
199.146029	525.687533	18.955303	-0.038358	1.453154
199.066846	517.884399	18.960307	-0.038338	1.445544
199.029081	510.092767	18.965312	-0.038327	1.437913
199.109803	502.281272	18.970317	-0.038337	1.430240
198.863846	494.521693	18.975322	-0.038286	1.422524
198.932760	486.719001	18.980327	-0.038294	1.414774
199.137873	478.895832	18.985331	-0.038328	1.406984
198.740006	471.180878	18.990336	-0.038249	1.399159
198.656331	463.407161	18.995341	-0.038228	1.391283
198.512224	455.627647	19.000346	-0.038197	1.383346
198.444572	447.857149	19.005351	-0.038179	1.375386
198.546922	440.063807	19.010355	-0.038193	1.367385
198.160837	432.358276	19.015360	-0.038117	1.359343
198.082185	424.609305	19.020365	-0.038097	1.351262
197.996964	416.847132	19.025370	-0.038077	1.343116
198.024537	409.081842	19.030375	-0.038077	1.334938
197.838651	401.348911	19.035379	-0.038038	1.326706
197.640294	393.631245	19.040384	-0.037996	1.318436
197.612011	385.802935	19.045389	-0.037986	1.310026
197.695379	377.994855	19.050394	-0.037996	1.301604
197.580701	370.287857	19.055399	-0.037970	1.293200
197.322482	362.599766	19.060403	-0.037918	1.284736
197.391586	354.866362	19.065408	-0.037926	1.276227
197.329518	347.162149	19.070413	-0.037909	1.267668
197.053994	339.493082	19.075418	-0.037853	1.259050
196.892831	331.799945	19.080423	-0.037818	1.250367
197.031865	324.079603	19.085427	-0.037840	1.241650
196.675157	316.439058	19.090432	-0.037768	1.232867
196.826287	308.698572	19.095437	-0.037792	1.224005
196.743115	301.028292	19.100442	-0.037772	1.215113
196.390504	293.388514	19.105447	-0.037701	1.206138
196.372348	285.728029	19.110451	-0.037693	1.197138
196.271322	278.061673	19.115456	-0.037670	1.188047
196.407898	270.380994	19.120461	-0.037690	1.178916
196.280497	262.742714	19.125466	-0.037662	1.169711
196.325308	255.086117	19.130471	-0.037665	1.160447
196.130967	247.470976	19.135475	-0.037624	1.151108
195.867252	239.844795	19.140480	-0.037571	1.141665
195.727588	232.248171	19.145485	-0.037540	1.132206
195.758935	224.613550	19.150490	-0.037541	1.122657
195.390667	217.068470	19.155495	-0.037468	1.113052
195.461547	209.445293	19.160499	-0.037476	1.103360
195.392591	201.856136	19.165504	-0.037459	1.093595
195.303941	194.287868	19.170509	-0.037438	1.083764
195.269833	186.723940	19.175514	-0.037427	1.073862
194.871780	179.207972	19.180519	-0.037348	1.063848
194.907158	171.645460	19.185523	-0.037350	1.053777
194.858057	164.098684	19.190528	-0.037336	1.043609
194.727574	156.596199	19.195533	-0.037307	1.033383
194.747116	149.059617	19.200538	-0.037306	1.023044
194.524185	141.588770	19.205543	-0.037260	1.012632
194.497209	134.098067	19.210547	-0.037250	1.002131
194.342941	126.620751	19.215552	-0.037217	0.991507
194.281100	119.136040	19.220557	-0.037201	0.980780
194.087943	111.706389	19.225562	-0.037160	0.969982
193.996946	104.273389	19.230567	-0.037139	0.959083
193.942493	96.856074	19.235571	-0.037124	0.948091
193.747721	89.472560	19.240576	-0.037083	0.936985
193.491915	82.112773	19.245581	-0.037031	0.925765
193.558072	74.720136	19.250586	-0.037039	0.914443
193.477194	67.356313	19.255591	-0.037019	0.902985
193.285297	60.277797	19.260595	-0.036979	0.891800