Thu Mar 11 19:09:31 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.538222	-0.057797	0.000000	0.000005	0.724890

0.355167	-0.029551	0.005005	0.000039	0.724881
0.368161	-0.025794	0.010010	0.000036	0.724894
0.279268	-0.015269	0.015014	0.000053	0.724884
0.358959	-0.027136	0.020019	0.000038	0.724889
0.483674	-0.049253	0.025024	0.000014	0.724890
0.306688	-0.022286	0.030029	0.000047	0.724881
0.470792	-0.047705	0.035034	0.000016	0.724889
0.243498	-0.009349	0.040038	0.000058	0.724885
0.278395	-0.013601	0.045043	0.000051	0.724890
0.387804	-0.032953	0.050048	0.000031	0.724890
0.377207	-0.035010	0.055053	0.000032	0.724883
0.380111	-0.029257	0.060058	0.000032	0.724896
0.432476	-0.043680	0.065062	0.000022	0.724886
0.416158	-0.039333	0.070067	0.000024	0.724890
0.394708	-0.037343	0.075072	0.000028	0.724886
0.452617	-0.050120	0.080077	0.000017	0.724882
0.527515	-0.168119	0.085082	0.000003	0.724678
0.375629	-0.186697	0.090086	0.000031	0.724589
0.387221	-0.186522	0.095091	0.000029	0.724594
0.342785	-0.177089	0.100096	0.000037	0.724597
0.376383	-0.187172	0.105101	0.000030	0.724590
0.179361	-0.148023	0.110106	0.000067	0.724598
0.393798	-0.223120	0.115110	0.000027	0.724526
0.517777	-0.382693	0.120115	0.000003	0.724257
0.374927	-0.354584	0.125120	0.000030	0.724263
0.403735	-0.364012	0.130125	0.000024	0.724255
0.415019	-0.361192	0.135130	0.000022	0.724265
0.358858	-0.402087	0.140134	0.000032	0.724166
0.411944	-0.521479	0.145139	0.000022	0.723951
0.386400	-0.514814	0.150144	0.000026	0.723956
0.316949	-0.506906	0.155149	0.000039	0.723947
0.310797	-0.514929	0.160154	0.000040	0.723930
0.336565	-0.674427	0.165158	0.000035	0.723627
0.473343	-0.697978	0.170163	0.000009	0.723629
0.182155	-0.645730	0.175168	0.000063	0.723630
0.321252	-0.723654	0.180173	0.000037	0.723526
0.502930	-0.851553	0.185178	0.000003	0.723340
0.332079	-0.823158	0.190182	0.000035	0.723336
0.078710	-0.778798	0.195187	0.000082	0.723335
0.229881	-0.968933	0.200192	0.000053	0.723015
0.187486	-0.971009	0.205197	0.000061	0.722997
0.212740	-0.971919	0.210202	0.000056	0.723005
0.188785	-1.098222	0.215206	0.000060	0.722749
0.308116	-1.151961	0.220211	0.000038	0.722686
0.281531	-1.144677	0.225216	0.000043	0.722691
0.096586	-1.264086	0.230221	0.000077	0.722392
0.094436	-1.276063	0.235226	0.000077	0.722369
0.149419	-1.302188	0.240230	0.000067	0.722337
0.009649	-1.412994	0.245235	0.000093	0.722071
0.127170	-1.433398	0.250240	0.000070	0.722073
0.070147	-1.498381	0.255245	0.000081	0.721925
-0.090801	-1.559700	0.260250	0.000111	0.721749
-0.174099	-1.549391	0.265254	0.000126	0.721741
-0.044577	-1.705971	0.270259	0.000102	0.721479
-0.045456	-1.727291	0.275264	0.000102	0.721437
-0.063179	-1.796863	0.280269	0.000105	0.721294
-0.050348	-1.886745	0.285274	0.000102	0.721123
0.008089	-1.911712	0.290278	0.000091	0.721094
-0.091697	-2.004527	0.295283	0.000109	0.720877
-0.143255	-1.994389	0.300288	0.000119	0.720880
0.141493	-2.197134	0.305293	0.000066	0.720581
-0.244050	-2.148142	0.310298	0.000137	0.720543
-0.583917	-2.205690	0.315302	0.000200	0.720311
-0.636520	-2.242102	0.320307	0.000210	0.720221
-1.270991	-2.203025	0.325312	0.000328	0.720076
-3.163344	-1.959608	0.330317	0.000680	0.719892
-2.860430	-2.010895	0.335322	0.000623	0.719898
-2.928990	-2.063609	0.340326	0.000636	0.719770
-3.989890	-1.963266	0.345331	0.000833	0.719596
-3.329541	-2.078489	0.350336	0.000710	0.719601
-3.809623	-2.013815	0.355341	0.000799	0.719561
-4.464885	-2.045972	0.360346	0.000921	0.719268
-4.503161	-2.042278	0.365350	0.000927	0.719262
-5.227652	-1.911860	0.370355	0.001062	0.719265
-4.768656	-2.035674	0.375360	0.000976	0.719183
-5.451890	-2.029136	0.380365	0.001103	0.718956
-5.520940	-2.013828	0.385370	0.001116	0.718963
-6.168936	-1.901660	0.390374	0.001236	0.718957
-5.628477	-1.997397	0.395379	0.001135	0.718958
-5.777581	-2.123166	0.400384	0.001163	0.718658
-6.984094	-1.920774	0.405389	0.001387	0.718634
-6.986651	-1.916439	0.410394	0.001388	0.718642
-6.221317	-2.054879	0.415398	0.001245	0.718638
-6.893346	-1.959702	0.420403	0.001370	0.718590
-7.562540	-1.958801	0.425408	0.001494	0.718357
-7.578190	-1.961069	0.430413	0.001497	0.718348
-7.617262	-1.950667	0.435418	0.001504	0.718355
-7.928517	-1.898626	0.440422	0.001561	0.718349
-7.765926	-1.926198	0.445427	0.001531	0.718352
-7.574027	-2.052423	0.450432	0.001495	0.718171
-8.964972	-1.886944	0.455437	0.001754	0.718009
-8.589754	-1.949346	0.460442	0.001684	0.718018
-8.454523	-1.977300	0.465446	0.001658	0.718011
-8.801957	-1.916086	0.470451	0.001723	0.718010
-8.461037	-1.972814	0.475456	0.001659	0.718018
-8.558782	-2.062969	0.480461	0.001677	0.717806
-9.427364	-1.961219	0.485466	0.001838	0.717702
-9.615788	-1.930774	0.490470	0.001873	0.717696
-9.569017	-1.937640	0.495475	0.001864	0.717700
-9.316483	-1.981432	0.500480	0.001817	0.717702
-9.504162	-1.953213	0.505485	0.001852	0.717693
-9.703554	-1.996311	0.510490	0.001889	0.717538
-10.549910	-1.928378	0.515494	0.002046	0.717374
-10.276130	-1.976508	0.520499	0.001995	0.717376
-10.478810	-1.939299	0.525504	0.002032	0.717379
-10.616973	-1.918909	0.530509	0.002058	0.717371
-10.024289	-2.019896	0.535514	0.001947	0.717380
-10.359807	-1.963169	0.540518	0.002009	0.717375
-11.136239	-1.968476	0.545523	0.002154	0.717091
-10.953104	-2.004762	0.550528	0.002119	0.717084
-11.337315	-1.941451	0.555533	0.002191	0.717075
-11.108419	-1.979418	0.560538	0.002148	0.717081
-10.942786	-2.012351	0.565542	0.002117	0.717074
-11.175381	-1.970522	0.570547	0.002160	0.717076
-10.969736	-2.096346	0.575552	0.002121	0.716900
-12.350255	-1.930460	0.580557	0.002378	0.716742
-11.689565	-2.043373	0.585562	0.002255	0.716752
-12.175245	-1.961431	0.590566	0.002345	0.716743
-12.420989	-1.916313	0.595571	0.002390	0.716746
-11.706803	-2.041081	0.600576	0.002257	0.716752
-11.889855	-2.015570	0.605581	0.002291	0.716738
-12.975637	-1.969220	0.610586	0.002493	0.716447
-12.963383	-1.974119	0.615590	0.002490	0.716442
-13.158560	-1.938797	0.620595	0.002527	0.716444
-12.886439	-1.984350	0.625600	0.002476	0.716450
-13.426489	-1.892641	0.630605	0.002576	0.716442
-12.977531	-1.969734	0.635610	0.002492	0.716448
-12.902407	-1.987567	0.640614	0.002478	0.716440
-13.639056	-1.983640	0.645619	0.002615	0.716188
-14.225422	-1.908618	0.650624	0.002724	0.716130
-13.975580	-1.956942	0.655629	0.002677	0.716123
-13.744637	-1.995045	0.660634	0.002634	0.716129
-13.914069	-1.967697	0.665638	0.002665	0.716124
-13.855382	-1.978778	0.670643	0.002654	0.716124
-13.872839	-1.973696	0.675648	0.002657	0.716128
-14.219512	-1.995180	0.680653	0.002721	0.715963
-14.645805	-1.961502	0.685658	0.002800	0.715880
-14.581154	-1.975931	0.690662	0.002788	0.715875
-14.990506	-1.904070	0.695667	0.002864	0.715873
-14.683227	-1.955339	0.700672	0.002807	0.715881
-14.552392	-1.983448	0.705677	0.002782	0.715872
-14.738953	-1.946391	0.710682	0.002816	0.715880
-15.129863	-2.034102	0.715686	0.002889	0.715568
-15.427541	-1.997053	0.720691	0.002944	0.715537
-15.386301	-2.001838	0.725696	0.002936	0.715542
-15.712753	-1.948522	0.730701	0.002997	0.715533
-15.395696	-2.000356	0.735706	0.002937	0.715543
-15.398111	-2.002088	0.740710	0.002938	0.715539
-15.717937	-2.001321	0.745715	0.002997	0.715428
-16.726278	-1.923771	0.750720	0.003184	0.715226
-16.562149	-1.954817	0.755725	0.003154	0.715223
-16.625737	-1.940260	0.760730	0.003165	0.715230
-16.780529	-1.916538	0.765734	0.003194	0.715223
-16.821505	-1.908488	0.770739	0.003201	0.715225
-16.517448	-1.960055	0.775744	0.003144	0.715230
-16.715537	-1.928265	0.780749	0.003181	0.715224
-16.645178	-2.056461	0.785754	0.003168	0.714995
-17.675231	-1.920153	0.790758	0.003359	0.714902
-17.812164	-1.895520	0.795763	0.003384	0.714903
-17.367217	-1.973684	0.800768	0.003301	0.714905
-17.573925	-1.942087	0.805773	0.003340	0.714895
-17.546146	-1.942038	0.810778	0.003334	0.714906
-17.484972	-1.956434	0.815782	0.003323	0.714899
-17.404383	-2.043462	0.820787	0.003307	0.714755
-18.354782	-1.950338	0.825792	0.003484	0.714605
-18.561182	-1.917889	0.830797	0.003522	0.714597
-18.584750	-1.909796	0.835802	0.003526	0.714605
-18.334747	-1.957242	0.840806	0.003480	0.714599
-18.427330	-1.940077	0.845811	0.003497	0.714601
-18.431152	-1.937271	0.850816	0.003497	0.714606
-18.284717	-2.010253	0.855821	0.003470	0.714513
-19.197979	-1.968159	0.860826	0.003639	0.714274
-19.036348	-1.999271	0.865830	0.003609	0.714270
-19.646328	-1.890477	0.870835	0.003722	0.714271
-19.287501	-1.951849	0.875840	0.003655	0.714276
-19.358861	-1.944713	0.880845	0.003668	0.714266
-19.199602	-1.968251	0.885850	0.003638	0.714276
-19.215224	-1.993166	0.890854	0.003641	0.714221
-20.369372	-1.918430	0.895859	0.003856	0.713962
-20.039049	-1.975943	0.900864	0.003794	0.713965
-20.487437	-1.898333	0.905869	0.003877	0.713961
-20.117111	-1.961953	0.910874	0.003808	0.713966
-20.406492	-1.914164	0.915878	0.003862	0.713959
-20.339616	-1.925959	0.920883	0.003849	0.713960
-20.037949	-1.975775	0.925888	0.003793	0.713968
-20.919203	-1.940065	0.930893	0.003956	0.713727
-21.626071	-1.852911	0.935898	0.004088	0.713651
-21.054432	-1.958132	0.940902	0.003981	0.713644
-21.182341	-1.936008	0.945907	0.004005	0.713643
-21.320602	-1.909410	0.950912	0.004030	0.713648
-21.385703	-1.900675	0.955917	0.004042	0.713643
-20.964937	-1.971203	0.960922	0.003963	0.713652
-21.192884	-1.947508	0.965926	0.004006	0.713619
-22.004706	-1.937013	0.970931	0.004157	0.713352
-21.810225	-1.969268	0.975936	0.004120	0.713358
-22.144294	-1.914807	0.980941	0.004182	0.713348
-21.887455	-1.957231	0.985946	0.004134	0.713355
-21.901545	-1.956680	0.990950	0.004136	0.713352
-22.266208	-1.892687	0.995955	0.004204	0.713350
-21.953153	-1.956977	1.000960	0.004146	0.713334
-22.566015	-2.010034	1.005965	0.004259	0.713011
-22.999825	-1.926463	1.010970	0.004340	0.713024
-23.255175	-1.883945	1.015974	0.004387	0.713019
-22.877258	-1.953161	1.020979	0.004317	0.713016
-22.888756	-1.947738	1.025984	0.004319	0.713023
-23.644078	-1.818412	1.030989	0.004459	0.713013
-22.988175	-1.932256	1.035994	0.004337	0.713019
-22.815431	-2.056288	1.040998	0.004304	0.712834
-24.224817	-1.870953	1.046003	0.004566	0.712704
-23.927168	-1.919791	1.051008	0.004511	0.712712
-24.071164	-1.899268	1.056013	0.004537	0.712703
-23.966794	-1.915981	1.061018	0.004518	0.712707
-23.585465	-1.985257	1.066022	0.004446	0.712705
-24.030837	-1.906683	1.071027	0.004529	0.712704
-23.939221	-1.994935	1.076032	0.004512	0.712561
-25.043906	-1.890350	1.081037	0.004717	0.712378
-24.657441	-1.954116	1.086042	0.004645	0.712388
-24.730081	-1.944423	1.091046	0.004658	0.712382
-24.991513	-1.899916	1.096051	0.004707	0.712379
-24.706198	-1.946677	1.101056	0.004653	0.712387
-24.998038	-1.898828	1.106061	0.004707	0.712379
-24.772361	-1.963018	1.111066	0.004665	0.712332
-25.675703	-1.925531	1.116070	0.004833	0.712086
-25.706846	-1.921155	1.121075	0.004839	0.712085
-25.602052	-1.937398	1.126080	0.004819	0.712090
-25.804872	-1.905800	1.131085	0.004856	0.712081
-25.553096	-1.946197	1.136090	0.004809	0.712091
-25.583868	-1.942984	1.141094	0.004815	0.712087
-25.536491	-1.971477	1.146099	0.004806	0.712047
-26.223369	-1.991965	1.151104	0.004933	0.711763
-26.665478	-1.916746	1.156109	0.005015	0.711756
-26.597000	-1.924054	1.161114	0.005002	0.711766
-26.341089	-1.974429	1.166118	0.004955	0.711757
-26.728056	-1.906883	1.171123	0.005026	0.711755
-26.619854	-1.921817	1.176128	0.005006	0.711764
-26.614093	-1.928753	1.181133	0.005005	0.711753
-27.118312	-1.983368	1.186138	0.005098	0.711465
-27.397284	-1.941599	1.191142	0.005150	0.711450
-27.744127	-1.881905	1.196147	0.005214	0.711446
-27.583267	-1.906068	1.201152	0.005184	0.711456
-27.556430	-1.918206	1.206157	0.005179	0.711441
-27.460910	-1.929865	1.211162	0.005161	0.711452
-27.842312	-1.864482	1.216166	0.005232	0.711448
-27.888997	-1.925689	1.221171	0.005240	0.711310
-28.240728	-1.948481	1.226176	0.005305	0.711140
-28.063201	-1.984496	1.231181	0.005272	0.711131
-28.393745	-1.921016	1.236186	0.005333	0.711141
-28.324697	-1.935705	1.241190	0.005320	0.711137
-28.320507	-1.938171	1.246195	0.005319	0.711134
-28.643127	-1.878333	1.251200	0.005379	0.711139
-28.887794	-1.888586	1.256205	0.005424	0.711032
-29.097069	-1.930941	1.261210	0.005463	0.710873
-29.095774	-1.933282	1.266214	0.005463	0.710869
-29.545543	-1.855985	1.271219	0.005546	0.710864
-29.068896	-1.936115	1.276224	0.005457	0.710874
-29.327283	-1.896246	1.281229	0.005505	0.710862
-29.401855	-1.878030	1.286234	0.005519	0.710873
-29.040691	-1.992273	1.291238	0.005451	0.710774
-30.085079	-1.926655	1.296243	0.005645	0.710533
-30.067575	-1.926882	1.301248	0.005642	0.710540
-30.291235	-1.893002	1.306253	0.005683	0.710528
-29.816774	-1.974114	1.311258	0.005595	0.710536
-29.980524	-1.946026	1.316262	0.005625	0.710534
-30.347070	-1.883010	1.321267	0.005693	0.710530
-29.813521	-2.056432	1.326272	0.005593	0.710374
-31.087512	-1.909866	1.331277	0.005830	0.710213
-30.946994	-1.931548	1.336282	0.005804	0.710221
-31.023856	-1.920584	1.341286	0.005818	0.710216
-31.367536	-1.859726	1.346291	0.005882	0.710215
-31.105417	-1.905305	1.351296	0.005833	0.710218
-31.540326	-1.832486	1.356301	0.005913	0.710209
-31.188144	-1.911496	1.361306	0.005847	0.710177
-31.691199	-1.966519	1.366310	0.005941	0.709888
-32.000852	-1.911725	1.371315	0.005998	0.709888
-31.957994	-1.916707	1.376320	0.005990	0.709894
-32.067362	-1.901978	1.381325	0.006010	0.709885
-32.085097	-1.894132	1.386330	0.006013	0.709895
-32.153418	-1.883322	1.391334	0.006026	0.709892
-31.720571	-1.963272	1.396339	0.005945	0.709887
-32.430764	-1.967619	1.401344	0.006077	0.709626
-33.145530	-1.859279	1.406349	0.006210	0.709588
-32.641193	-1.946116	1.411354	0.006116	0.709595
-32.510274	-1.971516	1.416358	0.006091	0.709591
-33.273435	-1.836794	1.421363	0.006233	0.709589
-32.685933	-1.936229	1.426368	0.006123	0.709600
-32.638463	-1.949254	1.431373	0.006114	0.709591
-33.473627	-1.948393	1.436378	0.006269	0.709296
-33.996664	-1.872378	1.441382	0.006367	0.709262
-33.571465	-1.948508	1.446387	0.006287	0.709262
-33.363361	-1.982593	1.451392	0.006248	0.709268
-34.105175	-1.855884	1.456397	0.006386	0.709258
-33.938590	-1.883116	1.461402	0.006355	0.709263
-33.544420	-1.953131	1.466406	0.006281	0.709264
-34.279132	-1.926430	1.471411	0.006418	0.709056
-34.874483	-1.868514	1.476416	0.006528	0.708960
-34.696590	-1.905014	1.481421	0.006495	0.708951
-34.577599	-1.923219	1.486426	0.006473	0.708957
-34.562263	-1.929032	1.491430	0.006469	0.708951
-34.770497	-1.893751	1.496435	0.006508	0.708948
-34.451164	-1.947740	1.501440	0.006448	0.708954
-34.880162	-1.930808	1.506445	0.006528	0.708836
-35.481151	-1.922844	1.511450	0.006640	0.708638
-35.114838	-1.989807	1.516454	0.006571	0.708635
-36.043021	-1.826404	1.521459	0.006744	0.708631
-35.577420	-1.905335	1.526464	0.006657	0.708640
-35.341948	-1.950731	1.531469	0.006613	0.708633
-35.324851	-1.949804	1.536474	0.006609	0.708642
-35.729536	-1.937215	1.541478	0.006684	0.708523
-36.348069	-1.915598	1.546483	0.006799	0.708346
-35.668552	-2.032192	1.551488	0.006673	0.708355
-36.488894	-1.892835	1.556493	0.006825	0.708342
-36.469678	-1.891002	1.561498	0.006821	0.708353
-36.128758	-1.953946	1.566502	0.006757	0.708349
-36.532075	-1.883931	1.571507	0.006832	0.708346
-36.437661	-2.013582	1.576512	0.006815	0.708120
-37.452457	-1.890215	1.581517	0.007003	0.708006
-37.268656	-1.920445	1.586522	0.006969	0.708011
-37.298213	-1.916228	1.591526	0.006974	0.708009
-37.539412	-1.875690	1.596531	0.007019	0.708005
-37.010067	-1.964199	1.601536	0.006920	0.708017
-37.428172	-1.895245	1.606541	0.006997	0.708007
-37.525169	-1.958846	1.611546	0.007015	0.707845
-37.917548	-1.962815	1.616550	0.007088	0.707697
-38.321653	-1.893939	1.621555	0.007163	0.707691
-38.415653	-1.873371	1.626560	0.007180	0.707699
-38.144983	-1.926557	1.631565	0.007130	0.707690
-38.055513	-1.939469	1.636570	0.007113	0.707696
-38.201691	-1.915088	1.641574	0.007140	0.707694
-38.427882	-1.920453	1.646579	0.007182	0.707602
-38.658308	-1.990096	1.651584	0.007224	0.707381
-38.924119	-1.949446	1.656589	0.007274	0.707368
-39.538866	-1.836292	1.661594	0.007388	0.707375
-39.187545	-1.899458	1.666598	0.007322	0.707375
-39.110368	-1.916599	1.671603	0.007307	0.707368
-39.089236	-1.915620	1.676608	0.007303	0.707378
-39.096129	-1.933528	1.681613	0.007304	0.707340
-39.330431	-2.021489	1.686618	0.007348	0.707081
-39.821478	-1.936876	1.691622	0.007439	0.707075
-40.356665	-1.842413	1.696627	0.007538	0.707074
-39.598151	-1.975324	1.701632	0.007397	0.707079
-40.061215	-1.897371	1.706637	0.007483	0.707070
-40.086378	-1.889193	1.711642	0.007487	0.707078
-39.619977	-2.013343	1.716646	0.007400	0.706996
-40.806225	-1.929297	1.721651	0.007621	0.706741
-40.805014	-1.925472	1.726656	0.007620	0.706749
-40.776659	-1.933636	1.731661	0.007615	0.706743
-40.411384	-1.994978	1.736666	0.007547	0.706752
-40.737416	-1.937912	1.741670	0.007607	0.706750
-41.122642	-1.869983	1.746675	0.007678	0.706749
-40.605878	-2.013855	1.751680	0.007582	0.706645
-41.824921	-1.900277	1.756685	0.007809	0.706437
-41.816571	-1.899280	1.761690	0.007807	0.706443
-41.448065	-1.967688	1.766694	0.007738	0.706438
-41.412341	-1.976115	1.771699	0.007731	0.706434
-41.485455	-1.960092	1.776704	0.007745	0.706441
-41.885544	-1.893396	1.781709	0.007819	0.706432
-41.638771	-1.994788	1.786714	0.007773	0.706317
-42.487187	-1.939847	1.791718	0.007930	0.706124
-42.531218	-1.935997	1.796723	0.007938	0.706116
-42.456064	-1.943882	1.801728	0.007924	0.706128
-42.668788	-1.910310	1.806733	0.007963	0.706120
-42.582912	-1.921970	1.811738	0.007947	0.706127
-42.522776	-1.934476	1.816742	0.007936	0.706124
-42.676063	-1.964295	1.821747	0.007964	0.706010
-43.499003	-1.892077	1.826752	0.008117	0.705861
-43.523381	-1.893127	1.831757	0.008121	0.705850
-43.211267	-1.946515	1.836762	0.008063	0.705855
-43.159467	-1.955013	1.841766	0.008053	0.705857
-43.679499	-1.863863	1.846771	0.008150	0.705855
-43.027398	-1.976811	1.851776	0.008028	0.705862
-43.266063	-2.022350	1.856781	0.008072	0.705685
-44.747374	-1.840446	1.861786	0.008348	0.705520
-44.206439	-1.937615	1.866790	0.008247	0.705519
-44.198467	-1.942645	1.871795	0.008245	0.705512
-44.125008	-1.950892	1.876800	0.008231	0.705522
-44.542168	-1.880638	1.881805	0.008309	0.705515
-44.323879	-1.914782	1.886810	0.008268	0.705525
-44.387186	-1.951825	1.891814	0.008279	0.705428
-45.728734	-1.824537	1.896819	0.008529	0.705203
-44.768492	-1.989830	1.901824	0.008350	0.705216
-45.077371	-1.940931	1.906829	0.008407	0.705204
-45.311726	-1.895082	1.911834	0.008450	0.705212
-45.159404	-1.924603	1.916838	0.008422	0.705208
-45.239717	-1.912961	1.921843	0.008437	0.705203
-45.132278	-1.979296	1.926848	0.008416	0.705109
-46.341857	-1.877958	1.931853	0.008641	0.704879
-45.732021	-1.986097	1.936858	0.008528	0.704881
-45.998016	-1.938367	1.941862	0.008577	0.704882
-46.519309	-1.846248	1.946867	0.008674	0.704880
-46.040434	-1.926506	1.951872	0.008584	0.704891
-46.082562	-1.924499	1.956877	0.008592	0.704881
-46.211253	-1.904619	1.961882	0.008616	0.704875
-46.756427	-1.949809	1.966886	0.008717	0.704589
-46.935475	-1.920291	1.971891	0.008750	0.704584
-46.667435	-1.963934	1.976896	0.008700	0.704593
-46.981148	-1.913197	1.981901	0.008758	0.704583
-47.106913	-1.889150	1.986906	0.008781	0.704587
-46.705380	-1.960542	1.991910	0.008706	0.704588
-47.091496	-1.912507	1.996915	0.008778	0.704546
-47.678619	-1.952305	2.001920	0.008887	0.704255

-48.030840	-1.889977	2.011917	0.008952	0.704255
-47.916073	-1.910633	2.021914	0.008930	0.704256
-48.033453	-1.890638	2.031910	0.008951	0.704255
-47.942240	-1.908180	2.041907	0.008934	0.704253
-47.739713	-1.943940	2.051904	0.008896	0.704255
-47.856841	-1.922091	2.061901	0.008917	0.704258
-47.912172	-1.913468	2.071898	0.008927	0.704256
-47.839727	-1.926579	2.081894	0.008913	0.704257
-47.872042	-1.921788	2.091891	0.008918	0.704256
-48.118456	-1.877470	2.101888	0.008964	0.704258
-47.836004	-1.928487	2.111885	0.008911	0.704257
-47.324840	-1.912727	2.121882	0.008815	0.704474
-47.019997	-1.911891	2.131878	0.008758	0.704586
-46.947199	-1.926305	2.141875	0.008744	0.704584
-47.020814	-1.911088	2.151872	0.008757	0.704589
-47.001970	-1.914177	2.161869	0.008753	0.704590
-47.016640	-1.906793	2.171866	0.008755	0.704601
-46.321413	-1.891198	2.181862	0.008625	0.704883
-46.180637	-1.916529	2.191859	0.008599	0.704884
-46.371919	-1.882507	2.201856	0.008634	0.704884
-46.245971	-1.906668	2.211853	0.008610	0.704882
-45.565431	-1.876944	2.221850	0.008483	0.705187
-45.413142	-1.895864	2.231846	0.008454	0.705204
-45.121923	-1.947509	2.241843	0.008399	0.705206
-45.524231	-1.865424	2.251840	0.008473	0.705228
-44.608913	-1.882172	2.261837	0.008303	0.705523
-44.398593	-1.920793	2.271834	0.008263	0.705522
-44.211969	-1.955732	2.281830	0.008228	0.705520
-44.312001	-1.913820	2.291827	0.008246	0.705569
-43.529383	-1.910213	2.301824	0.008100	0.705858
-43.303091	-1.949504	2.311821	0.008057	0.705861
-43.458192	-1.923021	2.321818	0.008085	0.705859
-43.618645	-1.845960	2.331814	0.008115	0.705958
-42.441319	-1.975492	2.341811	0.007895	0.706120
-42.816956	-1.907365	2.351808	0.007964	0.706124
-42.468292	-1.969129	2.361805	0.007899	0.706125
-42.061902	-1.921510	2.371802	0.007823	0.706368
-41.772852	-1.937840	2.381798	0.007769	0.706439
-41.848992	-1.925318	2.391795	0.007782	0.706438
-41.863804	-1.881295	2.401792	0.007785	0.706522
-41.047375	-1.914671	2.411789	0.007632	0.706748
-41.112667	-1.902449	2.421786	0.007644	0.706751
-41.151212	-1.895928	2.431782	0.007650	0.706751
-40.424810	-1.864949	2.441779	0.007515	0.707074
-40.258631	-1.892429	2.451776	0.007483	0.707079
-39.983739	-1.942673	2.461773	0.007432	0.707078
-39.780293	-1.891999	2.471770	0.007393	0.707253
-39.312397	-1.915935	2.481766	0.007306	0.707373
-39.398255	-1.902578	2.491763	0.007321	0.707370
-39.301773	-1.890097	2.501760	0.007303	0.707431
-38.342559	-1.929437	2.511757	0.007124	0.707696
-38.373204	-1.924325	2.521754	0.007129	0.707696
-38.415288	-1.917563	2.531750	0.007136	0.707696
-37.846728	-1.915905	2.541747	0.007030	0.707903
-37.697082	-1.891866	2.551744	0.007001	0.708006
-37.424540	-1.939506	2.561741	0.006950	0.708008
-37.539391	-1.896463	2.571738	0.006971	0.708055
-36.842634	-1.876688	2.581734	0.006841	0.708344
-36.617597	-1.918160	2.591731	0.006798	0.708342
-36.522845	-1.934033	2.601728	0.006780	0.708345
-36.039371	-1.927171	2.611725	0.006690	0.708533
-35.718458	-1.932749	2.621722	0.006630	0.708637
-35.955019	-1.891132	2.631718	0.006673	0.708637
-35.857230	-1.879060	2.641715	0.006654	0.708697
-35.106525	-1.884411	2.651712	0.006514	0.708955
-34.703089	-1.957444	2.661709	0.006439	0.708954
-34.909354	-1.919119	2.671706	0.006476	0.708958
-34.156660	-1.944687	2.681702	0.006336	0.709176
-33.984114	-1.931542	2.691699	0.006303	0.709265
-33.821059	-1.962943	2.701696	0.006272	0.709261
-33.934039	-1.941009	2.711693	0.006293	0.709265
-33.261853	-1.900136	2.721690	0.006167	0.709588
-33.180322	-1.910444	2.731686	0.006152	0.709597
-33.013544	-1.941297	2.741683	0.006120	0.709596
-32.910576	-1.896849	2.751680	0.006100	0.709722
-31.950028	-1.982980	2.761677	0.005921	0.709893
-32.290586	-1.921621	2.771674	0.005984	0.709896
-32.056856	-1.965969	2.781670	0.005940	0.709891
-31.712495	-1.883531	2.791667	0.005875	0.710180
-31.224655	-1.953650	2.801664	0.005784	0.710214
-31.380396	-1.927066	2.811661	0.005813	0.710213
-31.049528	-1.909130	2.821658	0.005750	0.710367
-30.390454	-1.945281	2.831654	0.005627	0.710531
-30.556273	-1.917411	2.841651	0.005658	0.710528
-30.332657	-1.955810	2.851648	0.005616	0.710532
-29.951678	-1.870755	2.861645	0.005544	0.710838
-29.594696	-1.918473	2.871642	0.005477	0.710871
-29.476558	-1.940031	2.881638	0.005455	0.710871
-29.738433	-1.831191	2.891635	0.005503	0.710996
-28.945716	-1.904158	2.901632	0.005355	0.711133
-29.064305	-1.882591	2.911629	0.005376	0.711135
-28.776117	-1.871003	2.921626	0.005322	0.711262
-28.212251	-1.877028	2.931622	0.005217	0.711451
-28.074736	-1.901685	2.941619	0.005191	0.711452
-27.785240	-1.941318	2.951616	0.005136	0.711476
-27.413762	-1.867131	2.961613	0.005067	0.711757
-27.064443	-1.928784	2.971610	0.005001	0.711759
-27.205483	-1.903923	2.981606	0.005027	0.711760
-26.699257	-1.884860	2.991603	0.004932	0.711978
-26.414387	-1.881344	3.001600	0.004879	0.712088
-26.454422	-1.874442	3.011597	0.004886	0.712088
-26.223557	-1.857882	3.021594	0.004842	0.712204
-25.432815	-1.908353	3.031590	0.004694	0.712385
-25.625622	-1.877132	3.041587	0.004730	0.712380
-25.502103	-1.895645	3.051584	0.004706	0.712388
-24.825391	-1.855712	3.061581	0.004580	0.712708
-24.377289	-1.936727	3.071578	0.004496	0.712707
-24.819405	-1.858064	3.081574	0.004578	0.712707
-24.244467	-1.877196	3.091571	0.004470	0.712874
-23.576409	-1.923266	3.101568	0.004345	0.713020
-23.761912	-1.889384	3.111565	0.004379	0.713023
-23.773787	-1.879763	3.121562	0.004381	0.713039
-22.775201	-1.898355	3.131558	0.004195	0.713357
-22.694643	-1.915060	3.141555	0.004179	0.713353
-22.717669	-1.911306	3.151552	0.004183	0.713353
-22.679423	-1.863616	3.161549	0.004175	0.713463
-21.634865	-1.956454	3.171546	0.003980	0.713649
-22.165911	-1.862620	3.181542	0.004079	0.713648
-21.804042	-1.927560	3.191539	0.004011	0.713648
-21.372593	-1.863714	3.201536	0.003930	0.713929
-20.997452	-1.912456	3.211533	0.003860	0.713966
-20.858330	-1.937512	3.221530	0.003833	0.713966
-21.058094	-1.847525	3.231526	0.003870	0.714075
-20.121496	-1.916473	3.241523	0.003695	0.714271
-20.290494	-1.885493	3.251520	0.003726	0.714273
-20.315870	-1.879078	3.261517	0.003730	0.714278
-19.403359	-1.876242	3.271514	0.003560	0.714607
-19.701500	-1.824381	3.281510	0.003615	0.714606
-19.090033	-1.934728	3.291507	0.003501	0.714604
-19.274602	-1.812673	3.301504	0.003535	0.714782
-18.483396	-1.890738	3.311501	0.003387	0.714908
-18.819073	-1.830852	3.321498	0.003449	0.714909
-18.453214	-1.842700	3.331494	0.003380	0.715016
-17.610454	-1.885447	3.341491	0.003223	0.715229
-17.701585	-1.868969	3.351488	0.003239	0.715231
-17.619685	-1.885326	3.361485	0.003224	0.715228
-16.967000	-1.859375	3.371482	0.003101	0.715511
-16.982511	-1.840011	3.381478	0.003104	0.715545
-16.704394	-1.891717	3.391475	0.003052	0.715542
-16.773484	-1.802808	3.401472	0.003064	0.715695
-15.429571	-1.947849	3.411469	0.002813	0.715883
-15.837114	-1.874651	3.421466	0.002889	0.715885
-15.391670	-1.957110	3.431462	0.002805	0.715879
-15.304758	-1.897491	3.441459	0.002789	0.716029
-14.899322	-1.919490	3.451456	0.002713	0.716130
-15.024847	-1.897714	3.461453	0.002735	0.716129
-14.851826	-1.924583	3.471450	0.002703	0.716138
-14.090301	-1.904955	3.481446	0.002561	0.716447
-13.962264	-1.930281	3.491443	0.002536	0.716442
-14.155774	-1.895172	3.501440	0.002572	0.716445
-13.531490	-1.935475	3.511437	0.002455	0.716586
-13.096432	-1.930250	3.521434	0.002374	0.716751
-13.185579	-1.914797	3.531430	0.002390	0.716751
-13.114027	-1.928996	3.541427	0.002376	0.716749
-12.348769	-1.924977	3.551424	0.002233	0.717027
-12.145181	-1.935477	3.561421	0.002194	0.717079
-12.197300	-1.927726	3.571418	0.002204	0.717077
-12.009365	-1.940097	3.581414	0.002168	0.717120
-11.631163	-1.881087	3.591411	0.002097	0.717371
-11.259175	-1.945282	3.601408	0.002028	0.717376
-11.234959	-1.949429	3.611405	0.002023	0.717377
-10.872496	-1.903736	3.621402	0.001955	0.717596
-10.345552	-1.946739	3.631398	0.001856	0.717697
-10.520713	-1.914306	3.641395	0.001888	0.717701
-10.272996	-1.943315	3.651392	0.001841	0.717731
-9.416338	-1.951803	3.661389	0.001681	0.718017
-9.357560	-1.962382	3.671386	0.001670	0.718018
-9.252962	-1.982784	3.681382	0.001650	0.718015
-9.523836	-1.880883	3.691379	0.001700	0.718122
-8.254107	-1.993452	3.701376	0.001463	0.718347
-8.503554	-1.946165	3.711373	0.001509	0.718354
-8.461809	-1.953988	3.721370	0.001501	0.718354
-7.854534	-1.977033	3.731366	0.001387	0.718523
-7.539742	-1.975562	3.741363	0.001328	0.718637
-7.614034	-1.961490	3.751360	0.001341	0.718640
-7.505020	-1.980698	3.761357	0.001321	0.718641
-6.861569	-1.963331	3.771354	0.001200	0.718903
-6.760210	-1.953486	3.781350	0.001181	0.718959
-6.785803	-1.949434	3.791347	0.001185	0.718959
-6.574669	-1.949947	3.801344	0.001146	0.719033
-6.020964	-1.931855	3.811341	0.001042	0.719264
-5.617185	-2.003321	3.821338	0.000966	0.719266
-5.751596	-1.979532	3.831334	0.000991	0.719266
-5.295609	-1.941696	3.841331	0.000905	0.719502
-4.862169	-1.970270	3.851328	0.000824	0.719599
-4.740374	-1.992585	3.861325	0.000801	0.719598
-4.759746	-1.985874	3.871322	0.000804	0.719606
-4.030006	-1.970867	3.881318	0.000668	0.719892
-3.872234	-1.999668	3.891315	0.000638	0.719892
-3.733052	-2.024564	3.901312	0.000612	0.719892
-3.985261	-1.927034	3.911309	0.000658	0.719997
-2.932859	-2.000955	3.921306	0.000462	0.720221
-3.083161	-1.975885	3.931302	0.000489	0.720219
-2.994310	-1.993047	3.941299	0.000472	0.720217
-2.531255	-1.957688	3.951296	0.000385	0.720450
-2.251661	-1.963834	3.961293	0.000333	0.720537
-2.375891	-1.942535	3.971290	0.000355	0.720536
-2.301851	-1.892810	3.981286	0.000341	0.720661
-1.837693	-1.868057	3.991283	0.000254	0.720873
-1.569350	-1.915673	4.001280	0.000204	0.720875
-1.638292	-1.870135	4.011277	0.000216	0.720941
-1.420486	-1.817840	4.021274	0.000175	0.721121
-1.451939	-1.814931	4.031270	0.000180	0.721117
-1.291627	-1.742359	4.041267	0.000150	0.721316
-1.284694	-1.682999	4.051264	0.000148	0.721436
-1.337797	-1.622244	4.061261	0.000158	0.721538
-1.223203	-1.538328	4.071258	0.000136	0.721744
-1.046520	-1.516916	4.081254	0.000102	0.721849
-0.904476	-1.428928	4.091251	0.000075	0.722072
-1.044728	-1.342142	4.101248	0.000101	0.722195
-0.841682	-1.289962	4.111245	0.000063	0.722369
-0.806271	-1.182786	4.121242	0.000055	0.722593
-0.723597	-1.135409	4.131238	0.000039	0.722715
-0.621460	-1.009022	4.141235	0.000020	0.723000
-0.547974	-0.931958	4.151232	0.000006	0.723178
-0.568007	-0.833797	4.161229	0.000009	0.723364
-0.504528	-0.709687	4.171226	-0.000004	0.723630
-0.506551	-0.592932	4.181222	-0.000004	0.723859
-0.475079	-0.486414	4.191219	-0.000010	0.724080
-0.389977	-0.382384	4.201216	-0.000027	0.724314
-0.290161	-0.260570	4.211213	-0.000046	0.724588
-0.406389	-0.092771	4.221210	-0.000025	0.724877
-0.149408	0.003491	4.231206	-0.000073	0.725156
-0.054530	0.127188	4.241203	-0.000091	0.725432
0.000000	0.270636	4.251200	-0.000102	0.725732

-0.048183	0.893929	4.256205	-0.000094	0.726932
0.112609	2.147524	4.261210	-0.000125	0.729430
0.357506	3.966057	4.266214	-0.000172	0.733042
0.680773	6.327737	4.271219	-0.000234	0.737707
0.945672	9.211826	4.276224	-0.000285	0.743321
1.476555	12.533348	4.281229	-0.000386	0.749810
2.047655	16.306915	4.286234	-0.000495	0.757103
2.190202	20.551120	4.291238	-0.000525	0.765058
2.828927	25.123740	4.296243	-0.000647	0.773695
3.550153	30.048094	4.301248	-0.000785	0.782901
4.411658	35.303990	4.306253	-0.000949	0.792636
5.424427	40.864206	4.311258	-0.001141	0.802839
6.576921	46.707264	4.316262	-0.001360	0.813448
7.413344	52.891274	4.321267	-0.001520	0.824412
7.938001	59.413698	4.326272	-0.001622	0.835711
9.182216	65.999689	4.331277	-0.001859	0.847179
10.411076	72.841641	4.336282	-0.002092	0.858911
11.138333	79.973625	4.341286	-0.002232	0.870812
11.887925	87.290604	4.346291	-0.002377	0.882856
13.106521	94.710072	4.351296	-0.002609	0.895030
14.379054	102.276336	4.356301	-0.002851	0.907285
14.850187	110.143488	4.361306	-0.002944	0.919622
15.371993	118.094355	4.366310	-0.003047	0.931937
16.987256	125.979511	4.371315	-0.003353	0.944280
18.023650	134.090357	4.376320	-0.003551	0.956646
18.861640	142.310642	4.381325	-0.003713	0.968964
19.787248	150.612297	4.386330	-0.003891	0.981266
20.406023	159.045269	4.391334	-0.004012	0.993527
21.316571	167.458726	4.396339	-0.004187	1.005681
22.092874	175.930793	4.401344	-0.004338	1.017739
22.863859	184.450676	4.406349	-0.004487	1.029720
23.931904	192.953414	4.411354	-0.004692	1.041610
24.831454	201.517925	4.416358	-0.004865	1.053408
25.534526	210.147318	4.421363	-0.005002	1.065116
26.205758	218.808976	4.426368	-0.005133	1.076732
27.239282	227.388953	4.431373	-0.005331	1.088199
28.095539	236.025766	4.436378	-0.005496	1.099579
28.733998	244.699234	4.441382	-0.005621	1.110841
29.393059	253.360752	4.446387	-0.005749	1.121979
29.959631	262.049840	4.451392	-0.005861	1.133022
30.552420	270.714004	4.456397	-0.005977	1.143933
31.709300	279.334790	4.461402	-0.006198	1.154805
32.155959	288.000535	4.466406	-0.006288	1.165483
32.832082	296.633783	4.471411	-0.006419	1.176071
33.748643	305.203683	4.476416	-0.006596	1.186538
34.504734	313.800039	4.481421	-0.006742	1.196912
35.470365	322.338813	4.486426	-0.006928	1.207171
35.983503	330.953848	4.491430	-0.007029	1.217342
36.719474	339.527836	4.496435	-0.007172	1.227424
37.453949	348.093235	4.501440	-0.007315	1.237414
37.911600	356.661153	4.506445	-0.007406	1.247274
38.652671	365.193598	4.511450	-0.007550	1.257069
39.570093	373.652025	4.516454	-0.007726	1.266740
40.259711	382.178917	4.521459	-0.007860	1.276369
40.934111	390.658577	4.526464	-0.007992	1.285872
41.379029	399.188564	4.531469	-0.008080	1.295317
42.189302	407.627678	4.536474	-0.008237	1.304662
42.752785	416.209368	4.541478	-0.008348	1.314049
43.280678	424.671429	4.546483	-0.008452	1.323234
44.190848	433.042296	4.551488	-0.008627	1.332328
44.823792	441.451311	4.556493	-0.008751	1.341350
45.431955	449.866104	4.561498	-0.008870	1.350314
45.856936	458.283501	4.566502	-0.008954	1.359189
46.541807	466.653697	4.571507	-0.009088	1.368002
47.191675	475.031741	4.576512	-0.009214	1.376761
47.860383	483.374211	4.581517	-0.009345	1.385430
48.623654	491.749272	4.586522	-0.009492	1.394095
49.032924	500.113132	4.591526	-0.009574	1.402635
49.581938	508.468047	4.596531	-0.009682	1.411138
50.509423	516.747823	4.601536	-0.009861	1.419577
51.038750	525.093034	4.606541	-0.009965	1.427965
51.460079	533.473200	4.611546	-0.010049	1.436321
51.940894	541.780635	4.616550	-0.010144	1.444567
52.650966	550.093121	4.621555	-0.010282	1.452808
53.228763	558.396364	4.626560	-0.010395	1.460971
53.701576	566.720100	4.631565	-0.010489	1.469093
54.143949	575.075087	4.636570	-0.010577	1.477194
54.511129	583.348784	4.641574	-0.010651	1.485162
55.161958	591.620594	4.646579	-0.010778	1.493130
55.636651	599.890161	4.651584	-0.010872	1.501025
56.209716	608.156637	4.656589	-0.010984	1.508892
56.984532	616.405260	4.661594	-0.011134	1.516731
57.435924	624.658979	4.666598	-0.011224	1.524486
57.882947	632.944921	4.671603	-0.011313	1.532230
58.278973	641.216158	4.676608	-0.011392	1.539914
58.500261	649.495664	4.681613	-0.011439	1.547541
59.312787	657.729881	4.686618	-0.011596	1.555177
59.356747	666.006551	4.691622	-0.011610	1.562701
59.740834	674.242328	4.696627	-0.011687	1.570202
60.201216	682.470735	4.701632	-0.011778	1.577671
60.725501	690.659939	4.706637	-0.011881	1.585079
61.496451	698.852997	4.711642	-0.012030	1.592491
61.848733	707.073445	4.716646	-0.012102	1.599833
62.436445	715.279622	4.721651	-0.012217	1.607163
62.899688	723.508342	4.726656	-0.012308	1.614461
63.050512	731.756956	4.731661	-0.012342	1.621699
63.533385	739.994580	4.736666	-0.012438	1.628942
63.950297	748.230752	4.741670	-0.012521	1.636143
64.511206	756.388707	4.746675	-0.012631	1.643264
64.628546	764.619358	4.751680	-0.012658	1.650356
64.977309	772.816057	4.756685	-0.012729	1.657420
65.266475	781.011744	4.761690	-0.012788	1.664445
65.411751	789.234108	4.766694	-0.012821	1.671443
65.794799	797.416804	4.771699	-0.012898	1.678411
66.382152	805.530620	4.776704	-0.013013	1.685319
66.556228	813.756617	4.781709	-0.013051	1.692238
66.771650	821.960143	4.786714	-0.013097	1.699115
67.076015	830.111853	4.791718	-0.013159	1.705933
67.621269	838.292581	4.796723	-0.013266	1.712780
67.710572	846.498366	4.801728	-0.013288	1.719560
67.939077	854.652360	4.806733	-0.013336	1.726289
68.704145	862.774494	4.811738	-0.013484	1.733035
69.048676	870.934189	4.816742	-0.013554	1.739731
69.138090	879.136180	4.821747	-0.013576	1.746403
69.358649	887.331766	4.826752	-0.013623	1.753062
69.543940	895.495388	4.831757	-0.013663	1.759665
69.805257	903.651744	4.836762	-0.013717	1.766246
70.223949	911.790847	4.841766	-0.013801	1.772809
70.617119	919.931169	4.846771	-0.013879	1.779346
70.693843	928.117525	4.851776	-0.013899	1.785856
71.056807	936.300717	4.856781	-0.013972	1.792375
71.550206	944.452216	4.861786	-0.014070	1.798861
71.461810	952.602435	4.866790	-0.014059	1.805252
71.953415	960.712818	4.871795	-0.014156	1.811659
72.311301	968.846187	4.876800	-0.014228	1.818046
72.458297	976.986914	4.881805	-0.014261	1.824391
72.638384	985.164583	4.886810	-0.014300	1.830746
72.950067	993.278099	4.891814	-0.014364	1.837045
73.164859	1001.412910	4.896819	-0.014409	1.843327
73.576667	1009.531614	4.901824	-0.014491	1.849599
73.856770	1017.674306	4.906829	-0.014549	1.855852
74.229101	1025.799423	4.911834	-0.014624	1.862082
74.324035	1033.953085	4.916838	-0.014647	1.868280
74.529354	1042.129915	4.921843	-0.014691	1.874488
75.098940	1050.188947	4.926848	-0.014803	1.880629
75.277411	1058.319400	4.931853	-0.014841	1.886758
75.480276	1066.480496	4.936858	-0.014885	1.892893
75.817589	1074.585871	4.941862	-0.014953	1.898982
76.202328	1082.676566	4.946867	-0.015030	1.905045
76.572438	1090.814802	4.951872	-0.015105	1.911123
76.617557	1098.979382	4.956877	-0.015119	1.917165
77.238561	1107.045056	4.961882	-0.015240	1.923179
77.535379	1115.165221	4.966886	-0.015301	1.929178
77.706627	1123.319612	4.971891	-0.015338	1.935170
78.153455	1131.406608	4.976896	-0.015427	1.941124
78.436592	1139.518950	4.981901	-0.015485	1.947060
78.774467	1147.692053	4.986906	-0.015554	1.953028
79.143735	1155.775346	4.991910	-0.015628	1.958917
79.711817	1163.830142	4.996915	-0.015739	1.964788
80.180230	1171.932907	5.001920	-0.015832	1.970666
80.243321	1180.086323	5.006925	-0.015849	1.976519
80.396946	1188.217471	5.011930	-0.015883	1.982348
80.611040	1196.329052	5.016934	-0.015929	1.988153
80.909105	1204.459756	5.021939	-0.015990	1.993963
81.220269	1212.545660	5.026944	-0.016053	1.999726
81.415382	1220.644276	5.031949	-0.016095	2.005469
81.585165	1228.782908	5.036954	-0.016132	2.011221
81.926488	1236.874913	5.041958	-0.016201	2.016942
82.514620	1244.935004	5.046963	-0.016316	2.022650
82.836111	1253.045375	5.051968	-0.016382	2.028349
82.909622	1261.215809	5.056973	-0.016401	2.034048
83.133819	1269.315294	5.061978	-0.016448	2.039698
83.500718	1277.360517	5.066982	-0.016522	2.045309
83.678202	1285.479008	5.071987	-0.016561	2.050935
84.358315	1293.533621	5.076992	-0.016693	2.056553
84.516104	1301.635588	5.081997	-0.016728	2.062136
84.723824	1309.754870	5.087002	-0.016772	2.067720
84.772827	1317.899084	5.092006	-0.016786	2.073291
85.233980	1325.950164	5.097011	-0.016878	2.078824
85.409486	1334.053829	5.102016	-0.016916	2.084349
85.666209	1342.141759	5.107021	-0.016969	2.089858
86.220131	1350.224301	5.112026	-0.017078	2.095377
86.483673	1358.295121	5.117030	-0.017133	2.100845
86.845317	1366.382288	5.122035	-0.017205	2.106320
87.143101	1374.548488	5.127040	-0.017266	2.111827
87.269048	1382.675786	5.132045	-0.017295	2.117277
87.667285	1390.721424	5.137050	-0.017375	2.122685
88.092989	1398.769624	5.142054	-0.017460	2.128083
88.328426	1406.883839	5.147059	-0.017509	2.133493
88.876508	1414.939513	5.152064	-0.017617	2.138881
88.866939	1423.055409	5.157069	-0.017620	2.144241
89.167241	1431.145843	5.162074	-0.017682	2.149601
89.443967	1439.237256	5.167078	-0.017739	2.154946
89.689844	1447.302851	5.172083	-0.017790	2.160257
89.920397	1455.397611	5.177088	-0.017839	2.165573
90.243654	1463.465957	5.182093	-0.017904	2.170868
90.546672	1471.577303	5.187098	-0.017966	2.176175
90.735349	1479.651028	5.192102	-0.018007	2.181435
90.867184	1487.744731	5.197107	-0.018037	2.186690
91.261891	1495.839180	5.202112	-0.018116	2.191956
91.406669	1503.934428	5.207117	-0.018149	2.197188
91.786106	1511.992144	5.212122	-0.018225	2.202404
91.840996	1520.080421	5.217126	-0.018240	2.207598
91.956758	1528.185336	5.222131	-0.018267	2.212796
92.364814	1536.242123	5.227136	-0.018349	2.217977
92.654244	1544.281723	5.232141	-0.018408	2.223125
92.902410	1552.385556	5.237146	-0.018460	2.228297
93.017506	1560.480708	5.242150	-0.018487	2.233441
93.430326	1568.538416	5.247155	-0.018569	2.238575
93.755063	1576.599250	5.252160	-0.018635	2.243691
93.860303	1584.681044	5.257165	-0.018660	2.248790
94.191040	1592.782954	5.262170	-0.018728	2.253910
94.474228	1600.843333	5.267174	-0.018786	2.258987
94.655301	1608.933740	5.272179	-0.018825	2.264063
94.791918	1617.029078	5.277184	-0.018856	2.269127
95.166836	1625.161570	5.282189	-0.018931	2.274223
95.337609	1633.223336	5.287194	-0.018969	2.279247
95.649044	1641.241249	5.292198	-0.019032	2.284244
96.092562	1649.276425	5.297203	-0.019120	2.289252
96.234236	1657.382718	5.302208	-0.019152	2.294267
96.650698	1665.401080	5.307213	-0.019235	2.299240
96.816304	1673.490866	5.312218	-0.019271	2.304226
96.885777	1681.576053	5.317222	-0.019290	2.309189
97.132955	1689.672251	5.322227	-0.019341	2.314163
97.407592	1697.722405	5.327232	-0.019398	2.319101
97.773802	1705.751257	5.332237	-0.019472	2.324023
98.082761	1713.827043	5.337242	-0.019535	2.328959
97.963845	1721.956522	5.342246	-0.019518	2.333881
98.243052	1730.010785	5.347251	-0.019576	2.338780
98.603163	1738.053050	5.352256	-0.019648	2.343668
98.730508	1746.129128	5.357261	-0.019677	2.348547
99.289357	1754.211505	5.362266	-0.019787	2.353454
99.492932	1762.261537	5.367270	-0.019830	2.358304
99.869032	1770.305008	5.372275	-0.019906	2.363153
100.193720	1778.368795	5.377280	-0.019972	2.368000
100.291390	1786.453684	5.382285	-0.019996	2.372832
100.798605	1794.494076	5.387290	-0.020095	2.377660
101.074252	1802.538307	5.392294	-0.020152	2.382462
101.449473	1810.615928	5.397299	-0.020228	2.387282
101.735475	1818.703321	5.402304	-0.020286	2.392090
101.821042	1826.773107	5.407309	-0.020308	2.396863
102.309965	1834.813209	5.412314	-0.020404	2.401641
102.557348	1842.865693	5.417318	-0.020456	2.406397
102.737699	1850.963956	5.422323	-0.020495	2.411166
102.939382	1859.053147	5.427328	-0.020538	2.415921
103.076911	1867.110546	5.432333	-0.020569	2.420644
103.350782	1875.173762	5.437338	-0.020626	2.425371
103.543686	1883.241338	5.442342	-0.020667	2.430085
103.851469	1891.372447	5.447347	-0.020730	2.434836
104.309765	1899.371627	5.452352	-0.020821	2.439512
104.456265	1907.418319	5.457357	-0.020854	2.444184
104.563960	1915.496423	5.462362	-0.020879	2.448861
104.779518	1923.569670	5.467366	-0.020925	2.453535
105.091606	1931.601311	5.472371	-0.020988	2.458183
105.307835	1939.662263	5.477376	-0.021034	2.462832
105.465412	1947.714388	5.482381	-0.021069	2.467463
105.844022	1955.804228	5.487386	-0.021145	2.472123
105.894681	1963.883119	5.492390	-0.021160	2.476743
106.086165	1971.907055	5.497395	-0.021201	2.481334
106.355460	1979.956738	5.502400	-0.021257	2.485937
106.363186	1988.026288	5.507405	-0.021264	2.490524
106.715370	1996.091756	5.512410	-0.021335	2.495124
107.185897	2004.121724	5.517414	-0.021428	2.499705
107.474745	2012.150087	5.522419	-0.021487	2.504264
107.680194	2020.233377	5.527424	-0.021531	2.508838
107.951111	2028.317309	5.532429	-0.021587	2.513410
108.382764	2036.361298	5.537434	-0.021673	2.517962
108.510112	2044.385916	5.542438	-0.021702	2.522474
108.784272	2052.430177	5.547443	-0.021758	2.526998
109.239199	2060.486044	5.552448	-0.021848	2.531534
109.499945	2068.538047	5.557453	-0.021903	2.536046
109.862369	2076.585708	5.562458	-0.021975	2.540555
110.049527	2084.633119	5.567462	-0.022016	2.545042
110.492334	2092.678692	5.572467	-0.022104	2.549539
110.647549	2100.787940	5.577472	-0.022138	2.554043
110.740044	2108.841308	5.582477	-0.022161	2.558504
111.001515	2116.877231	5.587482	-0.022215	2.562959
111.315403	2124.918134	5.592486	-0.022279	2.567413
111.566562	2132.992187	5.597491	-0.022331	2.571873
111.613454	2141.080540	5.602496	-0.022346	2.576318
111.650583	2149.129135	5.607501	-0.022358	2.580734
112.111308	2157.149216	5.612506	-0.022449	2.585156
112.396783	2165.190414	5.617510	-0.022508	2.589569
112.759280	2173.449262	5.622515	-0.022581	2.594099
113.015327	2181.458910	5.627520	-0.022634	2.598478
113.172482	2189.429330	5.632525	-0.022669	2.602821
113.460665	2197.452982	5.637530	-0.022728	2.607195
113.716019	2205.492355	5.642534	-0.022781	2.611568
113.950906	2213.548484	5.647539	-0.022830	2.615941
114.296412	2221.564312	5.652544	-0.022900	2.620292
114.443270	2229.598562	5.657549	-0.022933	2.624633
114.750928	2237.649561	5.662554	-0.022996	2.628987
114.801663	2245.729225	5.667558	-0.023011	2.633331
115.063707	2253.765948	5.672563	-0.023065	2.637659
115.449491	2261.793523	5.677568	-0.023142	2.641983
115.320411	2269.866449	5.682573	-0.023124	2.646291
115.810777	2277.898170	5.687578	-0.023220	2.650610
116.096794	2285.956873	5.692582	-0.023279	2.654923
116.238579	2294.003614	5.697587	-0.023311	2.659214
116.373604	2302.068973	5.702592	-0.023342	2.663506
116.760065	2310.079090	5.707597	-0.023419	2.667779
117.196260	2318.154072	5.712602	-0.023506	2.672082
117.163715	2326.236011	5.717606	-0.023505	2.676352
117.524794	2334.248784	5.722611	-0.023578	2.680604
117.669777	2342.279902	5.727616	-0.023610	2.684845
117.863296	2350.328637	5.732621	-0.023652	2.689092
118.367575	2358.382464	5.737626	-0.023751	2.693354
118.456894	2366.441545	5.742630	-0.023773	2.697586
118.306646	2374.506946	5.747635	-0.023751	2.701799
118.715951	2382.528429	5.752640	-0.023833	2.706018
119.030436	2390.552494	5.757645	-0.023897	2.710226
119.145312	2398.674865	5.762650	-0.023924	2.714466
119.162828	2406.694339	5.767654	-0.023932	2.718640
119.553941	2414.715268	5.772659	-0.024011	2.722831
119.957257	2422.741312	5.777664	-0.024091	2.727019
120.074563	2430.798258	5.782669	-0.024119	2.731199
120.223223	2438.897736	5.787674	-0.024152	2.735397
120.580550	2446.882148	5.792678	-0.024224	2.739541
120.888969	2454.910104	5.797683	-0.024287	2.743699
121.054784	2463.000043	5.802688	-0.024323	2.747873
121.109843	2471.094171	5.807693	-0.024339	2.752037
121.682230	2479.135432	5.812698	-0.024451	2.756198
121.939120	2487.132361	5.817702	-0.024504	2.760311
122.164050	2495.132909	5.822707	-0.024552	2.764418
122.451085	2503.192644	5.827712	-0.024610	2.768553
122.216654	2511.290061	5.832717	-0.024572	2.772670
122.609624	2519.315709	5.837722	-0.024651	2.776781
122.751169	2527.337330	5.842726	-0.024683	2.780870
122.885639	2535.366745	5.847731	-0.024713	2.784955
122.998877	2543.440692	5.852736	-0.024740	2.789056
123.469512	2551.451209	5.857741	-0.024833	2.793140
123.670662	2559.516664	5.862746	-0.024876	2.797230
123.717581	2567.541325	5.867750	-0.024890	2.801284
124.064813	2575.565302	5.872755	-0.024960	2.805350
124.518999	2583.604937	5.877760	-0.025050	2.809423
124.794609	2591.654043	5.882765	-0.025107	2.813485
124.923703	2599.726162	5.887770	-0.025137	2.817545
125.400024	2607.717847	5.892774	-0.025231	2.821578
125.613769	2615.762517	5.897779	-0.025276	2.825616
125.685123	2623.849466	5.902784	-0.025295	2.829662
125.992103	2631.903014	5.907789	-0.025358	2.833699
126.349587	2639.943669	5.912794	-0.025430	2.837726
126.670465	2647.944865	5.917798	-0.025495	2.841726
126.926935	2655.979914	5.922803	-0.025548	2.845734
127.145027	2664.028897	5.927808	-0.025594	2.849740
127.168784	2672.103107	5.932813	-0.025604	2.853742
127.411506	2680.139972	5.937818	-0.025655	2.857733
127.744336	2688.143287	5.942822	-0.025722	2.861706
127.883004	2696.182284	5.947827	-0.025754	2.865681
128.029170	2704.268457	5.952832	-0.025786	2.869674
128.408573	2712.292859	5.957837	-0.025862	2.873643
128.486366	2720.351507	5.962842	-0.025882	2.877608
128.609642	2728.379313	5.967846	-0.025911	2.881554
128.820487	2736.414173	5.972851	-0.025956	2.885503
129.311862	2744.442349	5.977856	-0.026052	2.889458
129.344093	2752.516829	5.982861	-0.026064	2.893406
129.601872	2760.559424	5.987866	-0.026117	2.897345
129.780040	2768.585387	5.992870	-0.026156	2.901266
130.106799	2776.590486	5.997875	-0.026222	2.905180
130.286633	2784.660696	6.002880	-0.026261	2.909112
130.360386	2792.784507	6.007885	-0.026281	2.913059
130.950259	2800.788531	6.012890	-0.026396	2.916971
131.062819	2808.797914	6.017894	-0.026422	2.920854
131.165189	2816.810739	6.022899	-0.026447	2.924733
131.629104	2824.821264	6.027904	-0.026539	2.928625
131.548761	2832.899514	6.032909	-0.026529	2.932516
131.813802	2840.944339	6.037914	-0.026584	2.936403
132.080893	2848.938680	6.042918	-0.026639	2.940261
132.269484	2856.961953	6.047923	-0.026680	2.944124
132.499611	2865.023289	6.052928	-0.026728	2.948002
132.845813	2873.046288	6.057933	-0.026798	2.951863
133.338874	2881.101354	6.062938	-0.026896	2.955741
133.382435	2889.116313	6.067942	-0.026909	2.959572
133.618770	2897.158928	6.072947	-0.026959	2.963421
133.901426	2905.175031	6.077952	-0.027017	2.967255
133.873145	2913.251403	6.082957	-0.027017	2.971097
134.209758	2921.311667	6.087962	-0.027085	2.974944
134.325313	2929.322566	6.092966	-0.027112	2.978752
134.741956	2937.347276	6.097971	-0.027195	2.982577
134.773355	2945.401072	6.102976	-0.027206	2.986391
134.827994	2953.413163	6.107981	-0.027222	2.990182
135.375601	2961.483094	6.112986	-0.027330	2.994020
135.722978	2969.492121	6.117990	-0.027400	2.997814
136.052653	2977.521314	6.122995	-0.027467	3.001612
136.517059	2985.559935	6.128000	-0.027559	3.005416
136.582238	2993.577192	6.133005	-0.027576	3.009186
136.932290	3001.637874	6.138010	-0.027647	3.012985
137.352744	3009.670205	6.143014	-0.027731	3.016769
137.570998	3017.699300	6.148019	-0.027777	3.020538
137.661748	3025.731144	6.153024	-0.027799	3.024296
137.780810	3033.780120	6.158029	-0.027827	3.028059
138.102040	3041.857001	6.163034	-0.027892	3.031841
138.440539	3049.879955	6.168038	-0.027961	3.035593
138.546275	3057.885432	6.173043	-0.027986	3.039321
138.512048	3065.935462	6.178048	-0.027985	3.043059
138.829194	3073.955044	6.183053	-0.028049	3.046795
139.132738	3081.979976	6.188058	-0.028111	3.050528
139.418594	3090.032248	6.193062	-0.028170	3.054268
139.720889	3098.065823	6.198067	-0.028232	3.057996
139.829944	3106.107520	6.203072	-0.028258	3.061713
139.820953	3114.136582	6.208077	-0.028261	3.065415
140.218232	3122.162351	6.213082	-0.028341	3.069130
140.581926	3130.243587	6.218086	-0.028414	3.072864
140.576750	3138.328177	6.223091	-0.028419	3.076578
140.996518	3146.305865	6.228096	-0.028502	3.080258
141.268784	3154.295996	6.233101	-0.028558	3.083933
141.712765	3162.313239	6.238106	-0.028647	3.087623
141.622658	3170.362797	6.243110	-0.028635	3.091300
142.023617	3178.396363	6.248115	-0.028715	3.094987
142.207087	3186.456798	6.253120	-0.028755	3.098672
142.198418	3194.483814	6.258125	-0.028759	3.102328
142.441483	3202.501265	6.263130	-0.028810	3.105987
142.659694	3210.539035	6.268134	-0.028856	3.109650
142.786895	3218.601676	6.273139	-0.028885	3.113316
143.129749	3226.626924	6.278144	-0.028954	3.116971
143.337799	3234.640682	6.283149	-0.028998	3.120609
143.614845	3242.657752	6.288154	-0.029056	3.124248
143.731648	3250.705022	6.293158	-0.029083	3.127890
143.957397	3258.748202	6.298163	-0.029130	3.131529
144.280997	3266.787748	6.303168	-0.029196	3.135168
144.398474	3274.788403	6.308173	-0.029223	3.138775
144.668506	3282.825715	6.313178	-0.029279	3.142402
144.896862	3290.857765	6.318182	-0.029327	3.146020
145.217676	3298.892227	6.323187	-0.029392	3.149639
145.322594	3306.989243	6.328192	-0.029417	3.153272
145.645448	3314.972538	6.333197	-0.029483	3.156860
145.892186	3323.010911	6.338202	-0.029534	3.160465
145.923709	3331.014434	6.343206	-0.029546	3.164041
146.243591	3339.019410	6.348211	-0.029611	3.167626
146.510968	3347.096883	6.353216	-0.029666	3.171237
146.550082	3355.128524	6.358221	-0.029679	3.174814
147.021578	3363.143781	6.363226	-0.029772	3.178397
147.189194	3371.167981	6.368230	-0.029809	3.181968
147.316726	3379.214988	6.373235	-0.029838	3.185543
147.377614	3387.260563	6.378240	-0.029855	3.189110
147.895031	3395.292056	6.383245	-0.029957	3.192687
148.339284	3403.336260	6.388250	-0.030045	3.196262
148.239382	3411.343832	6.393254	-0.030032	3.199794
148.627100	3419.342964	6.398259	-0.030109	3.203339
148.944237	3427.387617	6.403264	-0.030174	3.206896
148.918116	3435.415614	6.408269	-0.030174	3.210429
149.272734	3443.485456	6.413274	-0.030246	3.213991
149.482944	3451.511163	6.418278	-0.030291	3.217524
149.711027	3459.531307	6.423283	-0.030339	3.221052
149.815791	3467.556239	6.428288	-0.030364	3.224573
150.083151	3475.593346	6.433293	-0.030419	3.228101
150.300211	3483.675518	6.438298	-0.030465	3.231644
150.362605	3491.732445	6.443302	-0.030482	3.235165
150.630770	3499.693137	6.448307	-0.030537	3.238649
150.874801	3507.722839	6.453312	-0.030588	3.242158
150.989803	3515.738151	6.458317	-0.030615	3.245652
150.995614	3523.763629	6.463322	-0.030622	3.249142
151.388171	3531.790861	6.468326	-0.030700	3.252645
151.496737	3539.852349	6.473331	-0.030726	3.256147
151.681024	3547.863016	6.478336	-0.030766	3.259626
151.816980	3555.879553	6.483341	-0.030796	3.263103
152.155768	3563.936006	6.488346	-0.030865	3.266601
152.184373	3571.957259	6.493350	-0.030876	3.270067
152.514343	3579.992187	6.498355	-0.030943	3.273548
152.844687	3588.032178	6.503360	-0.031010	3.277027
152.978856	3596.035557	6.508365	-0.031040	3.280479
153.080129	3604.058400	6.513370	-0.031064	3.283935
153.408431	3612.079440	6.518374	-0.031131	3.287395
153.408534	3620.119002	6.523379	-0.031137	3.290846
153.807990	3628.181391	6.528384	-0.031216	3.294319
153.828398	3636.209179	6.533389	-0.031226	3.297759
154.282275	3644.232138	6.538394	-0.031316	3.301209
154.334355	3652.238205	6.543398	-0.031331	3.304634
154.588188	3660.266824	6.548403	-0.031384	3.308072
154.787698	3668.340239	6.553408	-0.031426	3.311524
154.802400	3676.359407	6.558413	-0.031434	3.314942
155.175882	3684.387406	6.563418	-0.031509	3.318374
155.221326	3692.391899	6.568422	-0.031523	3.321779
155.601162	3700.382532	6.573427	-0.031600	3.325188
155.693062	3708.445136	6.578432	-0.031622	3.328613
155.670956	3716.486310	6.583437	-0.031624	3.332022
156.136438	3724.498208	6.588442	-0.031716	3.335432
156.301955	3732.515934	6.593446	-0.031752	3.338830
156.181406	3740.561665	6.598451	-0.031735	3.342227
156.855234	3748.564973	6.603456	-0.031866	3.345630
156.997189	3756.562905	6.608461	-0.031898	3.349009
157.138472	3764.652075	6.613466	-0.031930	3.352423
157.339004	3772.691762	6.618470	-0.031972	3.355814
157.596004	3780.664995	6.623475	-0.032026	3.359176
157.816559	3788.721605	6.628480	-0.032072	3.362569
157.977016	3796.740258	6.633485	-0.032108	3.365939
158.592592	3804.736290	6.638490	-0.032228	3.369314
158.527462	3812.820375	6.643494	-0.032221	3.372697
158.739704	3820.886691	6.648499	-0.032266	3.376079
159.040169	3828.881964	6.653504	-0.032328	3.379432
159.189312	3836.873468	6.658509	-0.032361	3.382774
159.087260	3844.952609	6.663514	-0.032347	3.386140
159.205791	3852.958919	6.668518	-0.032375	3.389481
159.557000	3861.036887	6.673523	-0.032446	3.392856
159.755654	3869.085565	6.678528	-0.032488	3.396210
159.876131	3877.041346	6.683533	-0.032516	3.399520
160.077718	3885.041808	6.688538	-0.032559	3.402848
160.487483	3893.051672	6.693542	-0.032641	3.406183
160.586640	3901.080356	6.698547	-0.032665	3.409513
160.889974	3909.124143	6.703552	-0.032727	3.412852
161.029887	3917.159274	6.708557	-0.032758	3.416179
161.147698	3925.161788	6.713562	-0.032786	3.419488
161.152415	3933.181440	6.718566	-0.032792	3.422797
161.670561	3941.206794	6.723571	-0.032894	3.426123
161.779633	3949.247217	6.728576	-0.032920	3.429438
161.936012	3957.312105	6.733581	-0.032954	3.432762
162.155130	3965.360008	6.738586	-0.033001	3.436077
162.162773	3973.344783	6.743590	-0.033008	3.439356
162.421376	3981.354102	6.748595	-0.033061	3.442650
162.527276	3989.398844	6.753600	-0.033086	3.445951
162.567585	3997.410890	6.758605	-0.033099	3.449233
162.850897	4005.478945	6.763610	-0.033158	3.452542
162.962466	4013.524376	6.768614	-0.033184	3.455834
163.419891	4021.499269	6.773619	-0.033274	3.459105
163.575969	4029.556614	6.778624	-0.033309	3.462396
163.563665	4037.555443	6.783629	-0.033312	3.465655
164.056012	4045.601368	6.788634	-0.033409	3.468947
164.210327	4053.642117	6.793638	-0.033444	3.472222
164.428433	4061.698547	6.798643	-0.033490	3.475503
164.358222	4069.692410	6.803648	-0.033482	3.478745
164.587236	4077.686260	6.808653	-0.033530	3.481995
164.985183	4085.700598	6.813658	-0.033610	3.485255
165.034986	4093.732231	6.818662	-0.033624	3.488508
165.364077	4101.763410	6.823667	-0.033691	3.491766
165.562477	4109.806281	6.828672	-0.033734	3.495022
165.455055	4117.817919	6.833677	-0.033719	3.498253
165.731072	4125.844276	6.838682	-0.033776	3.501498
166.028137	4133.815340	6.843686	-0.033837	3.504719
166.223788	4141.876218	6.848691	-0.033879	3.507970
166.446123	4149.933293	6.853696	-0.033926	3.511217
166.662743	4157.923748	6.858701	-0.033971	3.514435
166.847796	4165.988639	6.863706	-0.034011	3.517678
167.032711	4174.018240	6.868710	-0.034051	3.520904
167.365321	4181.957485	6.873715	-0.034119	3.524095
167.560059	4190.028510	6.878720	-0.034160	3.527332
167.293240	4198.086683	6.883725	-0.034116	3.530547
167.835015	4206.093903	6.888730	-0.034222	3.533763
168.156463	4214.126901	6.893734	-0.034288	3.536979
168.329436	4222.140194	6.898739	-0.034325	3.540181
168.378974	4230.161492	6.903744	-0.034340	3.543378
168.617409	4238.195504	6.908749	-0.034390	3.546584
168.773499	4246.249347	6.913754	-0.034425	3.549792
168.938932	4254.369592	6.918758	-0.034461	3.553024
169.028951	4262.359753	6.923763	-0.034483	3.556199
169.532317	4270.311446	6.928768	-0.034582	3.559368
169.618642	4278.312385	6.933773	-0.034604	3.562542
169.612412	4286.361260	6.938778	-0.034608	3.565729
169.992142	4294.359693	6.943782	-0.034684	3.568904
170.201559	4302.394539	6.948787	-0.034729	3.572086
170.403410	4310.439580	6.953792	-0.034772	3.575269
170.490442	4318.425868	6.958797	-0.034794	3.578423
170.770614	4326.459047	6.963802	-0.034851	3.581597
170.853439	4334.464668	6.968806	-0.034872	3.584753
171.073708	4342.494409	6.973811	-0.034919	3.587919
171.380126	4350.577554	6.978816	-0.034981	3.591105
171.482473	4358.544386	6.983821	-0.035006	3.594238
171.588225	4366.601541	6.988826	-0.035031	3.597403
171.717132	4374.603648	6.993830	-0.035060	3.600544
171.742385	4382.594712	6.998835	-0.035070	3.603676
172.151190	4390.657944	7.003840	-0.035152	3.606843
172.133360	4398.656583	7.008845	-0.035154	3.609971
172.460985	4406.702395	7.013850	-0.035221	3.613124
172.534921	4414.758940	7.018854	-0.035240	3.616271
172.795058	4422.722924	7.023859	-0.035294	3.619385
173.040898	4430.759813	7.028864	-0.035345	3.622523
173.294278	4438.756738	7.033869	-0.035398	3.625644
173.614574	4446.812191	7.038874	-0.035463	3.628787
173.654123	4454.883925	7.043878	-0.035476	3.631925
173.861248	4462.900338	7.048883	-0.035520	3.635044
174.004794	4470.937807	7.053888	-0.035552	3.638167
174.199704	4478.933584	7.058893	-0.035594	3.641272
174.557731	4486.875033	7.063898	-0.035666	3.644358
174.677342	4494.913224	7.068902	-0.035694	3.647472
174.870744	4502.969437	7.073907	-0.035735	3.650592
175.317132	4511.043623	7.078912	-0.035824	3.653724
175.342126	4519.071164	7.083917	-0.035834	3.656823
175.485431	4527.095057	7.088922	-0.035866	3.659922
175.943048	4535.078565	7.093926	-0.035957	3.663010
176.103935	4543.109374	7.098931	-0.035992	3.666107
176.242861	4551.168017	7.103936	-0.036023	3.669211
176.384754	4559.176475	7.108941	-0.036055	3.672293
176.851996	4567.224403	7.113946	-0.036148	3.675396
176.874062	4575.216325	7.118950	-0.036157	3.678463
176.906876	4583.240287	7.123955	-0.036169	3.681541
177.082760	4591.237830	7.128960	-0.036207	3.684609
177.153961	4599.271095	7.133965	-0.036226	3.687686
177.276206	4607.324068	7.138970	-0.036254	3.690769
177.638114	4615.346795	7.143974	-0.036327	3.693843
177.887561	4623.348588	7.148979	-0.036379	3.696905
178.126764	4631.376634	7.153984	-0.036429	3.699973
178.226014	4639.359962	7.158989	-0.036453	3.703019
178.291745	4647.436564	7.163994	-0.036471	3.706097
178.538123	4655.424472	7.168998	-0.036522	3.709142
178.932900	4663.487496	7.174003	-0.036601	3.712218
179.282499	4671.557839	7.179008	-0.036671	3.715292
179.285115	4679.489496	7.184013	-0.036677	3.718303
179.484082	4687.531108	7.189018	-0.036720	3.721358
179.804460	4695.503256	7.194022	-0.036785	3.724387
179.971802	4703.527265	7.199027	-0.036822	3.727430
179.983378	4711.593402	7.204032	-0.036829	3.730482
180.272358	4719.606447	7.209037	-0.036889	3.733518
180.498374	4727.640875	7.214042	-0.036936	3.736558
180.547967	4735.627687	7.219046	-0.036951	3.739574
180.636594	4743.655794	7.224051	-0.036973	3.742603
181.054306	4751.670689	7.229056	-0.037056	3.745633
181.264590	4759.682806	7.234061	-0.037101	3.748655
181.276876	4767.796825	7.239066	-0.037108	3.751707
181.534263	4775.786774	7.244070	-0.037162	3.754717
181.571677	4783.802669	7.249075	-0.037174	3.757728
181.843753	4791.839691	7.254080	-0.037230	3.760750
181.884048	4799.833403	7.259085	-0.037243	3.763749
182.159628	4807.864959	7.264090	-0.037300	3.766764
182.411255	4815.876177	7.269094	-0.037352	3.769769
182.415472	4823.915633	7.274099	-0.037359	3.772777
182.706304	4831.975889	7.279104	-0.037418	3.775796
182.872711	4839.952407	7.284109	-0.037455	3.778779
182.969160	4847.998945	7.289114	-0.037478	3.781784
183.338395	4855.979432	7.294118	-0.037552	3.784768
183.556069	4864.005636	7.299123	-0.037598	3.787763
183.777723	4872.092591	7.304128	-0.037645	3.790778
183.580844	4880.116098	7.309133	-0.037614	3.793759
183.800197	4888.153099	7.314138	-0.037660	3.796751
184.082490	4896.089388	7.319142	-0.037718	3.799705
184.173496	4904.100474	7.324147	-0.037741	3.802680
184.561785	4912.138338	7.329152	-0.037819	3.805669
184.581535	4920.125860	7.334157	-0.037828	3.808628
184.820915	4928.163330	7.339162	-0.037878	3.811609
184.992008	4936.219614	7.344166	-0.037915	3.814593
184.885295	4944.223176	7.349171	-0.037901	3.817550
185.436165	4952.233005	7.354176	-0.038009	3.820520
185.532975	4960.228887	7.359181	-0.038032	3.823473
185.744770	4968.269295	7.364186	-0.038077	3.826443
185.780269	4976.308320	7.369190	-0.038089	3.829406
185.870589	4984.347082	7.374195	-0.038112	3.832368
186.199554	4992.358196	7.379200	-0.038178	3.835322
186.393331	5000.359494	7.384205	-0.038220	3.838268
186.273755	5008.415293	7.389210	-0.038203	3.841224
186.463227	5016.400342	7.394214	-0.038244	3.844159
186.656030	5024.369258	7.399219	-0.038285	3.847086
186.704979	5032.480178	7.404224	-0.038300	3.850060
186.887020	5040.496193	7.409229	-0.038339	3.852999
187.177793	5048.532024	7.414234	-0.038399	3.855946
187.427211	5056.534565	7.419238	-0.038451	3.858877
187.501068	5064.523896	7.424243	-0.038470	3.861798
187.757198	5072.573486	7.429248	-0.038523	3.864742
187.876613	5080.585430	7.434253	-0.038551	3.867667
187.965213	5088.651440	7.439258	-0.038573	3.870609
187.936466	5096.894616	7.444262	-0.038573	3.873611
188.306080	5104.856667	7.449267	-0.038647	3.876517
188.439617	5112.744821	7.454272	-0.038677	3.879388
188.699922	5120.720598	7.459277	-0.038731	3.882292
188.954381	5128.731159	7.464282	-0.038784	3.885206
189.172722	5136.731699	7.469286	-0.038830	3.888114
189.171927	5144.762010	7.474291	-0.038836	3.891026
189.332638	5152.857903	7.479296	-0.038871	3.893962
189.600054	5160.837916	7.484301	-0.038926	3.896857
189.805253	5168.816889	7.489306	-0.038970	3.899747
189.853645	5176.854993	7.494310	-0.038984	3.902654
190.071858	5184.847051	7.499315	-0.039031	3.905545
190.540205	5192.882339	7.504320	-0.039123	3.908455
190.685700	5200.909335	7.509325	-0.039156	3.911353
190.977543	5208.939154	7.514330	-0.039216	3.914253
191.145636	5216.943252	7.519334	-0.039252	3.917139
191.258213	5224.910177	7.524339	-0.039279	3.920008
191.412955	5232.971163	7.529344	-0.039313	3.922910
191.500230	5240.981648	7.534349	-0.039335	3.925790
191.706675	5248.993782	7.539354	-0.039379	3.928671
191.760038	5257.067463	7.544358	-0.039394	3.931570
191.980442	5265.058630	7.549363	-0.039441	3.934439
192.231324	5273.103022	7.554368	-0.039493	3.937326
192.342882	5281.084473	7.559373	-0.039519	3.940186
192.649832	5289.097889	7.564378	-0.039582	3.943058
192.776905	5297.122667	7.569382	-0.039611	3.945930
192.709428	5305.128819	7.574387	-0.039604	3.948789
193.075262	5313.179031	7.579392	-0.039677	3.951669
193.201345	5321.220705	7.584397	-0.039706	3.954540
193.344900	5329.236773	7.589402	-0.039739	3.957400
193.610588	5337.220361	7.594406	-0.039793	3.960249
193.786696	5345.236067	7.599411	-0.039832	3.963105
194.014564	5353.269204	7.604416	-0.039880	3.965966
194.130403	5361.251214	7.609421	-0.039907	3.968805
194.334712	5369.267321	7.614426	-0.039950	3.971656
194.474956	5377.327514	7.619430	-0.039982	3.974519
194.724197	5385.332087	7.624435	-0.040034	3.977362
194.935545	5393.350449	7.629440	-0.040078	3.980208
194.853617	5401.372501	7.634445	-0.040069	3.983048
195.202705	5409.412812	7.639450	-0.040139	3.985899
195.558607	5417.407500	7.644454	-0.040211	3.988732
195.591803	5425.460947	7.649459	-0.040223	3.991579
195.796746	5433.486613	7.654464	-0.040266	3.994416
195.648354	5441.530734	7.659469	-0.040244	3.997253
195.995322	5449.533109	7.664474	-0.040314	4.000080
196.101097	5457.542513	7.669478	-0.040339	4.002904
196.135963	5465.571476	7.674483	-0.040351	4.005732
196.366091	5473.591125	7.679488	-0.040400	4.008558
196.552649	5481.641585	7.684493	-0.040440	4.011392
196.832006	5489.645685	7.689498	-0.040497	4.014209
197.045467	5497.696708	7.694502	-0.040542	4.017039
196.989335	5505.642617	7.699507	-0.040537	4.019827
197.361939	5513.697147	7.704512	-0.040612	4.022657
197.489125	5521.693415	7.709517	-0.040641	4.025461
197.609897	5529.733061	7.714522	-0.040669	4.028278
197.694394	5537.796036	7.719526	-0.040691	4.031100
198.027397	5545.870024	7.724531	-0.040758	4.033928
198.013367	5553.875404	7.729536	-0.040761	4.036725
198.028871	5561.781317	7.734541	-0.040769	4.039486
198.374219	5569.842355	7.739546	-0.040839	4.042304
198.259312	5577.829323	7.744550	-0.040823	4.045087
198.392604	5585.847097	7.749555	-0.040853	4.047883
198.920205	5593.880771	7.754560	-0.040957	4.050688
199.052578	5601.891941	7.759565	-0.040987	4.053478
199.080270	5609.960665	7.764570	-0.040998	4.056284
199.252686	5617.908546	7.769574	-0.041035	4.059048
199.546972	5625.954919	7.774579	-0.041096	4.061846
199.689922	5633.945698	7.779584	-0.041128	4.064621
199.966355	5641.980669	7.784589	-0.041185	4.067411
200.160554	5650.014719	7.789594	-0.041226	4.070198
200.419014	5658.049953	7.794598	-0.041280	4.072984
200.314270	5666.045002	7.799603	-0.041266	4.075749
200.804680	5674.082941	7.804608	-0.041363	4.078536
200.620529	5682.093014	7.809613	-0.041334	4.081301
200.632064	5690.069915	7.814618	-0.041342	4.084056
200.852946	5698.092793	7.819622	-0.041388	4.086828
201.055975	5706.096563	7.824627	-0.041431	4.089591
201.307165	5714.195479	7.829632	-0.041484	4.092385
201.523510	5722.197115	7.834637	-0.041529	4.095144
201.901478	5730.212490	7.839642	-0.041605	4.097907
201.955771	5738.218701	7.844646	-0.041621	4.100662
201.766898	5746.177881	7.849651	-0.041591	4.103395
202.126588	5754.243164	7.854656	-0.041664	4.106169
202.549834	5762.248858	7.859661	-0.041748	4.108923
202.801721	5770.305745	7.864666	-0.041800	4.111689
203.126173	5778.356328	7.869670	-0.041866	4.114453
203.158414	5786.330411	7.874675	-0.041878	4.117185
203.519478	5794.324929	7.879680	-0.041950	4.119926
203.598744	5802.389241	7.884685	-0.041971	4.122685
203.723903	5810.373253	7.889690	-0.041999	4.125416
204.028287	5818.378897	7.894694	-0.042061	4.128155
203.917976	5826.422502	7.899699	-0.042046	4.130899
204.309603	5834.479751	7.904704	-0.042125	4.133653
204.258670	5842.527371	7.909709	-0.042121	4.136396
204.347357	5850.497391	7.914714	-0.042143	4.139112
204.613172	5858.526907	7.919718	-0.042198	4.141850
204.954083	5866.478410	7.924723	-0.042267	4.144559
204.964732	5874.566334	7.929728	-0.042274	4.147309
204.827578	5882.599573	7.934733	-0.042254	4.150037
205.195430	5890.578103	7.939738	-0.042328	4.152751
205.300907	5898.646591	7.944742	-0.042353	4.155490
205.366976	5906.589203	7.949747	-0.042371	4.158184
205.809739	5914.662292	7.954752	-0.042459	4.160926
205.807261	5922.615935	7.959757	-0.042464	4.163619
205.852140	5930.706925	7.964762	-0.042478	4.166358
206.071227	5938.658881	7.969766	-0.042524	4.169050
206.401158	5946.708446	7.974771	-0.042591	4.171775
206.625043	5954.764182	7.979776	-0.042638	4.174499
206.804872	5962.764754	7.984781	-0.042677	4.177201
207.151571	5970.753977	7.989786	-0.042747	4.179900
207.264839	5978.804338	7.994790	-0.042773	4.182615
207.199438	5986.756425	7.999795	-0.042767	4.185294
207.421235	5994.817446	8.004800	-0.042814	4.188010
207.737454	6002.839920	8.009805	-0.042878	4.190713
207.972226	6010.928831	8.014810	-0.042927	4.193435
208.008667	6018.975508	8.019814	-0.042939	4.196140
208.583988	6026.863421	8.024819	-0.043052	4.198795
208.579257	6034.944163	8.029824	-0.043057	4.201506
208.791202	6042.863200	8.034829	-0.043101	4.204164
209.059932	6050.913236	8.039834	-0.043157	4.206865
209.250115	6058.934621	8.044838	-0.043198	4.209554
209.052559	6066.972170	8.049843	-0.043167	4.212242
209.375686	6075.011997	8.054848	-0.043232	4.214935
209.402850	6082.984784	8.059853	-0.043243	4.217601
209.617910	6090.971942	8.064858	-0.043288	4.220271
209.672575	6099.043876	8.069862	-0.043304	4.222967
209.629398	6107.016263	8.074867	-0.043301	4.225626
209.824131	6115.084990	8.079872	-0.043343	4.228319
210.031236	6123.054559	8.084877	-0.043387	4.230976
210.152648	6131.120812	8.089882	-0.043415	4.233664
210.487142	6139.176709	8.094886	-0.043483	4.236348
210.691760	6147.115764	8.099891	-0.043526	4.238991
210.836628	6155.157402	8.104896	-0.043559	4.241665
210.854022	6163.084629	8.109901	-0.043568	4.244298
211.046293	6171.160517	8.114906	-0.043609	4.246981
211.172760	6179.197308	8.119910	-0.043638	4.249649
211.337836	6187.228719	8.124915	-0.043674	4.252313
211.804499	6195.270135	8.129920	-0.043766	4.254982
211.577251	6203.287665	8.134925	-0.043730	4.257634
211.792856	6211.291486	8.139930	-0.043775	4.260285
212.112082	6219.330646	8.144934	-0.043840	4.262946
212.219862	6227.302197	8.149939	-0.043866	4.265582
212.333036	6235.357062	8.154944	-0.043892	4.268244
212.388856	6243.368378	8.159949	-0.043908	4.270888
212.795950	6251.445555	8.164954	-0.043989	4.273557
212.817392	6259.481132	8.169958	-0.043999	4.276206
212.871785	6267.421332	8.174963	-0.044014	4.278822
213.159832	6275.483745	8.179968	-0.044074	4.281480
213.437577	6283.375979	8.184973	-0.044131	4.284079
213.573917	6291.496053	8.189978	-0.044162	4.286750
213.736535	6299.503720	8.194982	-0.044197	4.289384
213.745775	6307.552514	8.199987	-0.044204	4.292027
213.705175	6315.589432	8.204992	-0.044202	4.294665
214.229597	6323.550849	8.209997	-0.044305	4.297281
214.463951	6331.579612	8.215002	-0.044355	4.299915
214.539562	6339.587666	8.220006	-0.044374	4.302539
214.701332	6347.575704	8.225011	-0.044410	4.305156
214.709867	6355.631467	8.230016	-0.044417	4.307792
214.799555	6363.614834	8.235021	-0.044439	4.310404
214.882737	6371.668213	8.240026	-0.044460	4.313037
215.371637	6379.688520	8.245030	-0.044556	4.315660
215.429754	6387.687403	8.250035	-0.044573	4.318272
215.532183	6395.720789	8.255040	-0.044597	4.320893
215.539564	6403.709515	8.260045	-0.044604	4.323498
215.690679	6411.732454	8.265050	-0.044638	4.326113
215.933399	6419.781311	8.270054	-0.044688	4.328736
215.977276	6427.806880	8.275059	-0.044702	4.331348
216.356549	6435.785878	8.280064	-0.044778	4.333946
216.131949	6443.802978	8.285069	-0.044742	4.336550
216.505928	6451.797646	8.290074	-0.044817	4.339150
216.518790	6459.852023	8.295078	-0.044825	4.341765
216.598620	6467.770306	8.300083	-0.044845	4.344335
216.896064	6475.894907	8.305088	-0.044906	4.346971
217.062977	6483.873061	8.310093	-0.044942	4.349558
217.386917	6491.950236	8.315098	-0.045008	4.352176
217.436070	6500.025402	8.320102	-0.045023	4.354790
217.454132	6507.986356	8.325107	-0.045032	4.357365
217.781525	6515.952691	8.330112	-0.045098	4.359943
218.044879	6523.936728	8.335117	-0.045153	4.362524
218.077080	6531.930082	8.340122	-0.045164	4.365106
218.322060	6540.014109	8.345126	-0.045215	4.367716
218.484698	6548.001032	8.350131	-0.045251	4.370293
218.602967	6556.037174	8.355136	-0.045278	4.372884
218.535186	6564.033121	8.360141	-0.045271	4.375459
218.863862	6572.059454	8.365146	-0.045338	4.378045
219.090001	6580.062447	8.370150	-0.045385	4.380621
219.059306	6588.061274	8.375155	-0.045385	4.383193
219.250853	6596.104569	8.380160	-0.045426	4.385779
219.362626	6604.118124	8.385165	-0.045453	4.388354
219.621100	6612.141667	8.390170	-0.045506	4.390930
219.541064	6620.233297	8.395174	-0.045497	4.393526
219.763408	6628.190121	8.400179	-0.045544	4.396078
220.012158	6636.162917	8.405184	-0.045595	4.398634
220.012789	6644.201145	8.410189	-0.045601	4.401208
220.064437	6652.162259	8.415194	-0.045616	4.403756
220.229673	6660.267740	8.420198	-0.045652	4.406350
220.600789	6668.241904	8.425203	-0.045727	4.408901
220.582818	6676.325737	8.430208	-0.045729	4.411483
220.824188	6684.318308	8.435213	-0.045779	4.414036
221.059861	6692.351910	8.440218	-0.045829	4.416601
221.161323	6700.347288	8.445222	-0.045853	4.419151
221.389388	6708.368940	8.450227	-0.045901	4.421709
221.637939	6716.383267	8.455232	-0.045953	4.424263
221.591369	6724.351732	8.460237	-0.045950	4.426800
221.869009	6732.416248	8.465242	-0.046007	4.429367
222.141906	6740.503307	8.470246	-0.046063	4.431940
222.205672	6748.527379	8.475251	-0.046081	4.434490
222.414797	6756.518687	8.480256	-0.046125	4.437030
222.726481	6764.452263	8.485261	-0.046188	4.439549
222.721442	6772.523708	8.490266	-0.046193	4.442110
222.912226	6780.463258	8.495270	-0.046234	4.444628
223.045261	6788.547107	8.500275	-0.046264	4.447190
223.432712	6796.547589	8.505280	-0.046342	4.449726
223.370718	6804.611795	8.510285	-0.046336	4.452278
223.468894	6812.602590	8.515290	-0.046359	4.454806
223.725688	6820.657256	8.520294	-0.046413	4.457354
223.541215	6828.609329	8.525299	-0.046384	4.459866
223.932043	6836.685523	8.530304	-0.046462	4.462418
223.845718	6844.642494	8.535309	-0.046451	4.464929
224.003160	6852.669410	8.540314	-0.046486	4.467461
224.032788	6860.686556	8.545318	-0.046497	4.469989
224.091671	6868.728746	8.550323	-0.046514	4.472523
224.458962	6876.778093	8.555328	-0.046588	4.475059
224.384720	6884.748609	8.560333	-0.046579	4.477567
224.726353	6892.718175	8.565338	-0.046648	4.480075
224.958993	6900.750107	8.570343	-0.046697	4.482601
225.118825	6908.722804	8.575347	-0.046732	4.485106
225.206569	6916.835013	8.580352	-0.046754	4.487654
225.300429	6924.786628	8.585357	-0.046777	4.490150
225.625633	6932.832088	8.590362	-0.046843	4.492674
225.602297	6940.876527	8.595367	-0.046844	4.495196
225.625591	6948.877207	8.600371	-0.046854	4.497702
225.741497	6956.877542	8.605376	-0.046881	4.500208
225.841999	6964.877535	8.610381	-0.046905	4.502712
226.232543	6972.862548	8.615386	-0.046983	4.505210
226.397794	6980.933981	8.620391	-0.047020	4.507734
226.312560	6988.916118	8.625395	-0.047009	4.510227
226.521305	6997.038297	8.630400	-0.047054	4.512764
226.586610	7005.057188	8.635405	-0.047071	4.515266
226.787344	7013.005429	8.640410	-0.047114	4.517746
226.704901	7021.006325	8.645415	-0.047104	4.520240
227.077040	7028.980237	8.650419	-0.047179	4.522725
227.489258	7037.000528	8.655424	-0.047261	4.525223
227.362908	7045.038166	8.660429	-0.047243	4.527724
227.337105	7053.009250	8.665434	-0.047244	4.530203
227.581558	7061.101483	8.670439	-0.047295	4.532719
227.818290	7069.064679	8.675443	-0.047344	4.535194
227.867860	7077.117950	8.680448	-0.047359	4.537695
227.930298	7085.064925	8.685453	-0.047376	4.540161
228.069610	7093.099379	8.690458	-0.047407	4.542653
228.310072	7101.156890	8.695463	-0.047458	4.545151
228.439454	7109.131839	8.700467	-0.047487	4.547623
228.685973	7117.173108	8.705472	-0.047539	4.550113
228.838806	7125.229442	8.710477	-0.047573	4.552606
228.844710	7133.228364	8.715482	-0.047579	4.555081
228.988788	7141.241117	8.720487	-0.047611	4.557558
229.035347	7149.211216	8.725491	-0.047626	4.560021
229.151443	7157.284464	8.730496	-0.047653	4.562514
229.459653	7165.245059	8.735501	-0.047715	4.564971
229.675549	7173.285336	8.740506	-0.047761	4.567452
229.533601	7181.333386	8.745511	-0.047740	4.569933
229.523976	7189.315383	8.750515	-0.047744	4.572392
230.027847	7197.392318	8.755520	-0.047843	4.574880
230.118452	7205.375666	8.760525	-0.047866	4.577337
230.125776	7213.343279	8.765530	-0.047872	4.579788
230.104659	7221.457441	8.770535	-0.047874	4.582283
230.516589	7229.395105	8.775539	-0.047956	4.584723
230.764505	7237.441241	8.780544	-0.048008	4.587194
230.652498	7245.430494	8.785549	-0.047992	4.589647
230.640641	7253.533732	8.790554	-0.047996	4.592133
230.802818	7261.562661	8.795559	-0.048031	4.594595
230.978149	7269.568436	8.800563	-0.048069	4.597048
231.216919	7277.480610	8.805568	-0.048119	4.599472
231.265700	7285.564551	8.810573	-0.048134	4.601947
231.289669	7293.484489	8.815578	-0.048144	4.604370
231.594214	7301.578965	8.820583	-0.048206	4.606845
231.653410	7309.516606	8.825587	-0.048222	4.609271
231.781878	7317.662893	8.830592	-0.048252	4.611760
232.050045	7325.641794	8.835597	-0.048307	4.614196
232.280173	7333.657768	8.840602	-0.048356	4.616642
232.348530	7341.650395	8.845607	-0.048374	4.619080
232.488076	7349.632972	8.850611	-0.048405	4.621513
232.695304	7357.619865	8.855616	-0.048449	4.623946
232.755530	7365.689891	8.860621	-0.048466	4.626404
232.704057	7373.674848	8.865626	-0.048462	4.628834
232.879059	7381.744357	8.870631	-0.048500	4.631288
233.059269	7389.748382	8.875635	-0.048539	4.633722
233.232172	7397.796762	8.880640	-0.048577	4.636167
233.172146	7405.740036	8.885645	-0.048571	4.638580
233.515958	7413.775709	8.890650	-0.048640	4.641018
234.028210	7421.740988	8.895655	-0.048741	4.643435
234.018665	7429.782468	8.900659	-0.048745	4.645873
234.259100	7437.832960	8.905664	-0.048795	4.648312
234.313695	7445.880039	8.910669	-0.048811	4.650750
234.512176	7453.888480	8.915674	-0.048853	4.653174
234.750319	7461.919888	8.920679	-0.048903	4.655604
234.824254	7469.875518	8.925683	-0.048922	4.658010
234.963355	7477.925419	8.930688	-0.048954	4.660443
235.122506	7485.890767	8.935693	-0.048989	4.662849
235.288900	7493.867566	8.940698	-0.049025	4.665257
235.482640	7501.965607	8.945703	-0.049067	4.667701
235.549443	7509.937999	8.950707	-0.049085	4.670105
235.515780	7518.103639	8.955712	-0.049084	4.672567
235.788232	7526.138238	8.960717	-0.049140	4.674987
235.757026	7534.051166	8.965722	-0.049140	4.677370
235.713394	7542.033423	8.970727	-0.049137	4.679773
235.997030	7550.016341	8.975731	-0.049195	4.682174
236.247537	7557.996020	8.980736	-0.049247	4.684573
236.401053	7566.021939	8.985741	-0.049281	4.686985
236.591484	7574.047081	8.990746	-0.049322	4.689395
236.808933	7582.107806	8.995751	-0.049368	4.691815
236.708594	7590.071899	9.000755	-0.049355	4.694205
236.974178	7598.160075	9.005760	-0.049410	4.696630
237.226863	7606.108687	9.010765	-0.049462	4.699012
237.143820	7614.131033	9.015770	-0.049452	4.701415
237.270575	7622.145398	9.020775	-0.049482	4.703815
237.274193	7630.191184	9.025779	-0.049488	4.706223
237.608624	7638.204959	9.030784	-0.049555	4.708620
237.721550	7646.203491	9.035789	-0.049582	4.711011
237.842715	7654.280399	9.040794	-0.049610	4.713424
238.038329	7662.292053	9.045799	-0.049652	4.715816
238.024818	7670.231853	9.050803	-0.049655	4.718187
238.422621	7678.298453	9.055808	-0.049734	4.720592
238.323895	7686.303237	9.060813	-0.049721	4.722980
238.478119	7694.336289	9.065818	-0.049756	4.725374
238.685771	7702.359291	9.070823	-0.049800	4.727763
238.967515	7710.313713	9.075827	-0.049858	4.730131
238.923290	7718.390872	9.080832	-0.049855	4.732535
239.012289	7726.391529	9.085837	-0.049877	4.734915
239.145111	7734.364124	9.090842	-0.049907	4.737284
239.405201	7742.457647	9.095847	-0.049961	4.739689
239.330661	7750.438407	9.100851	-0.049953	4.742059
239.542910	7758.450327	9.105856	-0.049998	4.744437
239.577022	7766.481303	9.110861	-0.050009	4.746820
239.709520	7774.434212	9.115866	-0.050040	4.749178
239.910501	7782.506723	9.120871	-0.050082	4.751570
239.962252	7790.513200	9.125875	-0.050098	4.753942
240.061079	7798.572753	9.130880	-0.050121	4.756328
240.050599	7806.529617	9.135885	-0.050125	4.758683
240.493412	7814.521108	9.140890	-0.050213	4.761045
240.759804	7822.557936	9.145895	-0.050268	4.763420
240.667851	7830.551193	9.150899	-0.050256	4.765783
241.040941	7838.560490	9.155904	-0.050331	4.768147
241.009881	7846.596335	9.160909	-0.050331	4.770519
241.301562	7854.615956	9.165914	-0.050391	4.772885
241.350193	7862.705351	9.170919	-0.050405	4.775270
241.345006	7870.602122	9.175923	-0.050410	4.777598
241.511977	7878.638598	9.180928	-0.050446	4.779965
241.723128	7886.679728	9.185933	-0.050491	4.782332
241.800732	7894.627609	9.190938	-0.050511	4.784671
242.263674	7902.729151	9.195943	-0.050603	4.787053
242.256495	7910.700826	9.200947	-0.050607	4.789397
242.131082	7918.777785	9.205952	-0.050589	4.791771
242.324586	7926.741088	9.210957	-0.050630	4.794109
242.474946	7934.822595	9.215962	-0.050664	4.796481
242.548455	7942.758044	9.220967	-0.050683	4.798810
242.697652	7950.752824	9.225971	-0.050716	4.801154
242.884776	7958.787308	9.230976	-0.050757	4.803509
242.853509	7966.822430	9.235981	-0.050756	4.805863
243.022173	7974.801718	9.240986	-0.050793	4.808200
243.221213	7982.867583	9.245991	-0.050836	4.810560
243.258251	7990.324412	9.250995	-0.050848	4.812741
243.341215	7994.936926	9.256000	-0.050866	4.814090

243.480572	7997.239937	9.261005	-0.050894	4.814763
243.667149	7998.723963	9.266010	-0.050930	4.815196
243.618058	7999.156718	9.271015	-0.050921	4.815323
243.614872	7999.745072	9.276019	-0.050921	4.815495
243.815700	7999.807099	9.281024	-0.050959	4.815512
243.719988	7999.794882	9.286029	-0.050941	4.815509
243.584744	7999.774546	9.291034	-0.050917	4.815503
243.863702	7999.782316	9.296039	-0.050969	4.815504
243.696843	7999.708071	9.301043	-0.050938	4.815483
243.835367	7999.756268	9.306048	-0.050964	4.815497
243.968402	7999.748847	9.311053	-0.050989	4.815494
244.016289	7999.772074	9.316058	-0.050998	4.815501
243.915712	7999.809968	9.321063	-0.050980	4.815512
243.981439	7999.758734	9.326067	-0.050992	4.815497
244.194486	7999.847659	9.331072	-0.051032	4.815522
244.116741	7999.806901	9.336077	-0.051018	4.815510
244.389887	7999.776134	9.341082	-0.051069	4.815500
244.463043	7999.870255	9.346087	-0.051083	4.815527
244.264373	7999.767724	9.351091	-0.051046	4.815498
244.411984	7999.824614	9.356096	-0.051074	4.815514
244.576227	7999.837992	9.361101	-0.051105	4.815517
244.423693	7999.809897	9.366106	-0.051076	4.815510
244.432446	7999.853845	9.371111	-0.051078	4.815523
244.441259	7999.805954	9.376115	-0.051080	4.815508
244.469057	7999.857688	9.381120	-0.051086	4.815523
244.656117	7999.826586	9.386125	-0.051121	4.815513
244.599486	7999.823548	9.391130	-0.051110	4.815513
244.776543	7999.865969	9.396135	-0.051144	4.815524
244.784064	7999.850094	9.401139	-0.051145	4.815520
244.645591	7999.846790	9.406144	-0.051120	4.815519
244.719642	7999.865105	9.411149	-0.051134	4.815524
244.687879	7999.860337	9.416154	-0.051128	4.815523
244.803549	7999.918844	9.421159	-0.051150	4.815540
244.747401	7999.837856	9.426163	-0.051140	4.815516
245.036075	7999.869283	9.431168	-0.051194	4.815524
244.839583	7999.825519	9.436173	-0.051157	4.815512
244.897036	7999.825410	9.441178	-0.051168	4.815512
245.215050	7999.864790	9.446183	-0.051228	4.815522
245.037700	7999.808524	9.451187	-0.051195	4.815506
245.012102	7999.809195	9.456192	-0.051190	4.815507
244.879355	7999.906368	9.461197	-0.051166	4.815536
244.951979	7999.808258	9.466202	-0.051180	4.815507
245.057241	7999.921059	9.471207	-0.051200	4.815539
244.927346	7999.899739	9.476211	-0.051176	4.815533
245.242919	7999.835492	9.481216	-0.051235	4.815513
245.242403	7999.915599	9.486221	-0.051235	4.815537
245.142345	7999.820012	9.491226	-0.051216	4.815509
245.217964	7999.899224	9.496231	-0.051231	4.815532
245.173919	7999.967942	9.501235	-0.051223	4.815552
244.997748	7999.836941	9.506240	-0.051190	4.815515
245.168962	7999.849365	9.511245	-0.051222	4.815518
245.299112	7999.932671	9.516250	-0.051247	4.815541
245.351650	7999.824621	9.521255	-0.051257	4.815509
245.321726	7999.886094	9.526259	-0.051251	4.815528
245.403018	7999.938702	9.531264	-0.051267	4.815542
245.314648	7999.834761	9.536269	-0.051251	4.815513
245.148829	7999.889746	9.541274	-0.051220	4.815529
245.380906	7999.915979	9.546279	-0.051263	4.815536
245.393147	7999.801932	9.551283	-0.051266	4.815503
245.136878	7999.845831	9.556288	-0.051219	4.815517
245.206434	7999.913197	9.561293	-0.051232	4.815536
245.529997	7999.826655	9.566298	-0.051292	4.815509
245.525342	7999.944072	9.571303	-0.051292	4.815543
245.503515	7999.840148	9.576307	-0.051288	4.815513
245.435590	7999.920224	9.581312	-0.051275	4.815537
245.630345	7999.996042	9.586317	-0.051312	4.815558
245.442564	7999.828539	9.591322	-0.051277	4.815510
245.565775	7999.850861	9.596327	-0.051300	4.815516
245.486555	7999.834639	9.601331	-0.051286	4.815512
245.515611	7999.893870	9.606336	-0.051291	4.815529
245.573887	7999.912997	9.611341	-0.051303	4.815534
245.580454	7999.855457	9.616346	-0.051304	4.815517
245.717774	7999.948493	9.621351	-0.051330	4.815544
245.459439	7999.841779	9.626355	-0.051282	4.815514
245.720538	7999.839652	9.631360	-0.051331	4.815512
245.606720	7999.895485	9.636365	-0.051310	4.815529
245.341874	7999.905069	9.641370	-0.051261	4.815533
245.646770	7999.897249	9.646375	-0.051318	4.815529
245.545366	7999.909499	9.651379	-0.051299	4.815533
245.597152	7999.836678	9.656384	-0.051309	4.815512
245.812015	7999.945930	9.661389	-0.051349	4.815542
245.709498	7999.849232	9.666394	-0.051330	4.815515
245.859643	7999.915779	9.671399	-0.051359	4.815533
245.763594	7999.865109	9.676403	-0.051341	4.815519
245.751325	7999.859590	9.681408	-0.051339	4.815518
245.749398	7999.998412	9.686413	-0.051339	4.815558
245.559990	7999.854376	9.691418	-0.051304	4.815517
245.377705	7999.875987	9.696423	-0.051270	4.815524
245.502910	7999.904748	9.701427	-0.051294	4.815532
245.619287	7999.836185	9.706432	-0.051316	4.815511
245.666197	7999.846583	9.711437	-0.051325	4.815514
245.554572	7999.897112	9.716442	-0.051304	4.815529
245.642324	7999.945554	9.721447	-0.051321	4.815543
245.742526	7999.850028	9.726451	-0.051340	4.815515
245.916503	7999.949001	9.731456	-0.051372	4.815543
246.015960	7999.923947	9.736461	-0.051391	4.815535
245.877434	7999.905689	9.741466	-0.051365	4.815530
245.805048	7999.875696	9.746471	-0.051352	4.815522
245.808158	7999.975086	9.751475	-0.051353	4.815551
245.970241	7999.924355	9.756480	-0.051383	4.815535
245.841658	7999.894512	9.761485	-0.051360	4.815527
245.727821	7999.836076	9.766490	-0.051339	4.815511
246.014826	7999.887768	9.771495	-0.051392	4.815524
246.076949	7999.937929	9.776499	-0.051404	4.815539
246.002403	7999.843823	9.781504	-0.051391	4.815512
245.864384	7999.965473	9.786509	-0.051365	4.815548
245.969623	7999.845467	9.791514	-0.051385	4.815512
245.965072	7999.903082	9.796519	-0.051384	4.815529
246.077661	7999.868631	9.801523	-0.051406	4.815518
246.135144	7999.882405	9.806528	-0.051417	4.815522
245.967248	7999.954443	9.811533	-0.051386	4.815544
245.918910	7999.850086	9.816538	-0.051377	4.815514
246.039947	7999.932177	9.821543	-0.051400	4.815537
246.092793	7999.863645	9.826547	-0.051410	4.815517
246.013554	7999.890140	9.831552	-0.051395	4.815525
246.363158	7999.990913	9.836557	-0.051461	4.815553
246.215912	7999.896688	9.841562	-0.051433	4.815526
246.158803	7999.895778	9.846567	-0.051423	4.815526
246.028574	7999.849889	9.851571	-0.051399	4.815513
246.159198	7999.842430	9.856576	-0.051423	4.815510
246.003207	7999.941361	9.861581	-0.051395	4.815540
245.724049	7999.922944	9.866586	-0.051343	4.815536
246.101998	7999.919520	9.871591	-0.051414	4.815533
246.023306	7999.909714	9.876595	-0.051399	4.815531
246.062361	7999.874063	9.881600	-0.051407	4.815520
246.091701	7999.882039	9.886605	-0.051412	4.815522
246.063771	7999.860245	9.891610	-0.051407	4.815516
246.116512	7999.918796	9.896615	-0.051418	4.815533
246.108626	7999.956067	9.901619	-0.051416	4.815544
246.127742	7999.883780	9.906624	-0.051420	4.815523
246.094557	7999.918502	9.911629	-0.051414	4.815533
246.107767	7999.871750	9.916634	-0.051417	4.815519
246.232109	8000.042536	9.921639	-0.051440	4.815568
246.180257	7999.946663	9.926643	-0.051431	4.815541
246.123387	7999.907311	9.931648	-0.051421	4.815529
246.029362	7999.869488	9.936653	-0.051403	4.815519
246.225355	7999.890862	9.941658	-0.051440	4.815524
246.255005	7999.899911	9.946663	-0.051446	4.815527
246.122755	7999.870008	9.951667	-0.051421	4.815518
246.342760	7999.894978	9.956672	-0.051463	4.815525
246.427446	7999.920944	9.961677	-0.051479	4.815532
246.287483	7999.879167	9.966682	-0.051453	4.815520
246.258517	7999.936385	9.971687	-0.051448	4.815537
246.242555	7999.953233	9.976691	-0.051445	4.815542
246.278754	7999.850255	9.981696	-0.051452	4.815512
246.066189	7999.870303	9.986701	-0.051413	4.815519
246.297282	7999.908269	9.991706	-0.051456	4.815529
246.349593	7999.887785	9.996711	-0.051466	4.815523
246.194417	7999.888478	10.001715	-0.051437	4.815523
246.298493	7999.951071	10.006720	-0.051457	4.815541
246.292137	7999.850601	10.011725	-0.051456	4.815512
246.299034	7999.833648	10.016730	-0.051457	4.815507
246.199965	7999.971954	10.021735	-0.051439	4.815548
246.249566	7999.909776	10.026739	-0.051449	4.815529
246.208818	7999.889909	10.031744	-0.051441	4.815524
246.269722	7999.884517	10.036749	-0.051453	4.815522
246.224584	7999.876326	10.041754	-0.051445	4.815520
246.369235	8000.022881	10.046759	-0.051472	4.815562
246.359287	7999.863615	10.051763	-0.051470	4.815515
246.468621	7999.906003	10.056768	-0.051491	4.815527
246.334122	7999.912373	10.061773	-0.051466	4.815530
246.440552	7999.878889	10.066778	-0.051486	4.815519
246.257899	7999.915444	10.071783	-0.051452	4.815531
246.362409	7999.884064	10.076787	-0.051472	4.815521
246.483865	7999.913834	10.081792	-0.051495	4.815529
246.459310	7999.982872	10.086797	-0.051491	4.815550
246.589624	7999.929487	10.091802	-0.051515	4.815533
246.747138	7999.964118	10.096807	-0.051545	4.815543
246.142069	7999.909410	10.101811	-0.051432	4.815530
246.440240	7999.929249	10.106816	-0.051488	4.815534
246.455816	7999.925252	10.111821	-0.051491	4.815533
246.459449	7999.897566	10.116826	-0.051492	4.815525
246.491424	7999.946167	10.121831	-0.051498	4.815539
246.397934	7999.905149	10.126835	-0.051481	4.815527
246.508795	7999.960377	10.131840	-0.051502	4.815543
246.668531	7999.943782	10.136845	-0.051532	4.815537
246.519351	7999.923214	10.141850	-0.051505	4.815532
246.494726	7999.952736	10.146855	-0.051500	4.815541
246.367756	7999.926122	10.151859	-0.051477	4.815533
246.660786	7999.903159	10.156864	-0.051532	4.815525
246.503403	7999.950806	10.161869	-0.051503	4.815540
246.577303	7999.892228	10.166874	-0.051517	4.815523
246.413411	7999.928021	10.171879	-0.051486	4.815534
246.445981	7999.881584	10.176883	-0.051493	4.815520
246.383175	7999.838930	10.181888	-0.051481	4.815508
246.328405	7999.948057	10.186893	-0.051471	4.815540
246.377856	7999.838886	10.191898	-0.051481	4.815508
246.634506	7999.925328	10.196903	-0.051529	4.815532
246.569930	7999.901869	10.201907	-0.051517	4.815525
246.581172	7999.901006	10.206912	-0.051519	4.815525
246.624943	7999.992518	10.211917	-0.051528	4.815552
246.570931	7999.854959	10.216922	-0.051518	4.815512
246.623673	7999.950890	10.221927	-0.051528	4.815539
246.486562	7999.947605	10.226931	-0.051503	4.815539
246.596517	7999.954761	10.231936	-0.051523	4.815541
246.716846	7999.947135	10.236941	-0.051546	4.815538
246.627926	7999.932889	10.241946	-0.051530	4.815534
246.684791	7999.958402	10.246951	-0.051540	4.815541
246.595489	7999.925995	10.251955	-0.051524	4.815532
246.847390	7999.902360	10.256960	-0.051571	4.815524
246.728014	7999.936744	10.261965	-0.051549	4.815535
246.670362	7999.873883	10.266970	-0.051539	4.815517
246.560660	7999.936191	10.271975	-0.051519	4.815535
246.580075	7999.957889	10.276979	-0.051522	4.815542
246.644070	7999.900217	10.281984	-0.051535	4.815524
246.498205	7999.905334	10.286989	-0.051508	4.815527
246.655375	7999.926075	10.291994	-0.051537	4.815532
246.882965	7999.999229	10.296999	-0.051580	4.815552
246.823314	7999.945947	10.302003	-0.051569	4.815537
246.787592	7999.912278	10.307008	-0.051563	4.815527
246.822542	7999.964132	10.312013	-0.051569	4.815542
246.804986	7999.935032	10.317018	-0.051566	4.815534
246.917980	7999.964665	10.322023	-0.051588	4.815542
246.716626	7999.917613	10.327027	-0.051550	4.815529
246.660490	7999.923126	10.332032	-0.051540	4.815531
246.686690	7999.952410	10.337037	-0.051545	4.815539
246.637518	7999.914250	10.342042	-0.051536	4.815528
246.719978	7999.970084	10.347047	-0.051552	4.815544
246.683036	7999.940667	10.352051	-0.051545	4.815536
246.711174	7999.955031	10.357056	-0.051551	4.815540
246.767164	7999.938879	10.362061	-0.051561	4.815535
246.621052	7999.924768	10.367066	-0.051534	4.815532
246.743743	7999.960967	10.372071	-0.051558	4.815542
246.687509	7999.941915	10.377075	-0.051547	4.815536
246.729045	7999.968245	10.382080	-0.051555	4.815544
246.656348	7999.967080	10.387085	-0.051542	4.815544
246.636831	7999.989210	10.392090	-0.051539	4.815550
246.802301	8000.003680	10.397095	-0.051570	4.815554
246.780340	7999.945673	10.402099	-0.051566	4.815537
246.788715	7999.962918	10.407104	-0.051568	4.815542
246.780414	7999.961736	10.412109	-0.051566	4.815542
246.721841	7999.922355	10.417114	-0.051556	4.815530
246.726840	7999.945953	10.422119	-0.051557	4.815537
246.732202	7999.940722	10.427123	-0.051558	4.815536
246.805545	7999.861843	10.432128	-0.051572	4.815512
246.917473	7999.926702	10.437133	-0.051593	4.815531
246.772244	7999.914741	10.442138	-0.051566	4.815528
246.877421	7999.992305	10.447143	-0.051586	4.815550
246.612136	7999.962365	10.452147	-0.051537	4.815542
246.517613	7999.932008	10.457152	-0.051520	4.815534
246.828409	8000.042832	10.462157	-0.051578	4.815565
246.771789	7999.857170	10.467162	-0.051567	4.815511
246.853541	7999.972798	10.472167	-0.051583	4.815544
246.885202	7999.976541	10.477171	-0.051589	4.815545
247.062015	7999.968769	10.482176	-0.051622	4.815542
246.784328	7999.956781	10.487181	-0.051571	4.815540
246.899013	7999.967219	10.492186	-0.051592	4.815542
247.192039	8000.020083	10.497191	-0.051647	4.815557
247.112486	7999.949387	10.502195	-0.051633	4.815536
246.999570	7999.979604	10.507200	-0.051612	4.815546
247.064855	7999.957196	10.512205	-0.051624	4.815539
247.002229	7999.915612	10.517210	-0.051613	4.815527
246.965198	7999.994059	10.522215	-0.051606	4.815550
246.830557	7999.921396	10.527219	-0.051581	4.815529
246.900165	7999.958865	10.532224	-0.051594	4.815540
246.881752	7999.942566	10.537229	-0.051591	4.815535
246.726415	7999.959275	10.542234	-0.051563	4.815541
246.874371	7999.992683	10.547239	-0.051590	4.815550
246.984326	7999.969936	10.552243	-0.051611	4.815543
246.904062	7999.922724	10.557248	-0.051596	4.815529
246.879197	7999.938359	10.562253	-0.051592	4.815534
246.928955	7999.906086	10.567258	-0.051602	4.815524
246.970955	7999.897181	10.572263	-0.051610	4.815522
246.932726	7999.921142	10.577267	-0.051603	4.815529
247.016799	7999.875545	10.582272	-0.051619	4.815515
247.034908	7999.948484	10.587277	-0.051622	4.815536
246.808046	7999.898879	10.592282	-0.051580	4.815523
247.017654	7999.952517	10.597287	-0.051620	4.815537
246.922073	7999.947774	10.602291	-0.051602	4.815537
246.877657	7999.965226	10.607296	-0.051594	4.815542
246.800518	7999.975736	10.612301	-0.051580	4.815545
246.834053	7999.945333	10.617306	-0.051586	4.815536
247.120433	7999.943622	10.622311	-0.051640	4.815534
246.996603	7999.888223	10.627315	-0.051617	4.815519
247.083277	7999.885388	10.632320	-0.051633	4.815518
247.126183	7999.954460	10.637325	-0.051642	4.815537
247.047443	7999.936108	10.642330	-0.051627	4.815532
247.145991	7999.968710	10.647335	-0.051646	4.815542
247.052972	7999.890318	10.652339	-0.051629	4.815519
246.961145	7999.913404	10.657344	-0.051612	4.815526
246.898148	7999.932689	10.662349	-0.051600	4.815532
247.047492	7999.913788	10.667354	-0.051628	4.815526
246.995076	7999.956741	10.672359	-0.051619	4.815539
247.003170	7999.919516	10.677363	-0.051621	4.815528
246.818425	7999.947492	10.682368	-0.051587	4.815537
247.223020	7999.980818	10.687373	-0.051662	4.815545
246.890481	8000.011722	10.692378	-0.051601	4.815555
247.201684	8000.028572	10.697383	-0.051659	4.815559
246.909532	7999.942657	10.702387	-0.051605	4.815535
246.987093	7999.975984	10.707392	-0.051619	4.815544
247.071386	7999.972042	10.712397	-0.051635	4.815543
247.249326	8000.016620	10.717402	-0.051669	4.815555
247.186143	8000.022017	10.722407	-0.051657	4.815557
247.017490	7999.921031	10.727411	-0.051626	4.815528
247.064753	7999.965611	10.732416	-0.051635	4.815541
247.089631	7999.968175	10.737421	-0.051640	4.815542
247.087879	7999.959624	10.742426	-0.051640	4.815539
247.210458	7999.983006	10.747431	-0.051663	4.815545
247.189196	7999.957049	10.752435	-0.051659	4.815538
247.072452	7999.980795	10.757440	-0.051638	4.815545
246.944214	7999.979791	10.762445	-0.051614	4.815546
246.977423	7999.945112	10.767450	-0.051620	4.815535
247.098969	7999.979157	10.772455	-0.051643	4.815545
247.105098	7999.964326	10.777459	-0.051645	4.815540
247.159684	7999.929996	10.782464	-0.051655	4.815530
247.251481	7999.982779	10.787469	-0.051672	4.815545
247.196969	7999.958415	10.792474	-0.051662	4.815538
247.176980	7999.965586	10.797479	-0.051659	4.815540
247.169405	7999.914220	10.802483	-0.051658	4.815525
247.377392	7999.929385	10.807488	-0.051697	4.815529
247.193763	7999.938156	10.812493	-0.051663	4.815532
247.237620	7999.967729	10.817498	-0.051671	4.815541
247.608361	8000.002640	10.822503	-0.051741	4.815549
247.257764	7999.923246	10.827507	-0.051675	4.815528
247.133500	7999.909491	10.832512	-0.051653	4.815524
247.140955	7999.950217	10.837517	-0.051654	4.815536
247.021362	7999.934402	10.842522	-0.051632	4.815532
247.173685	7999.970018	10.847527	-0.051661	4.815542
247.143438	7999.966341	10.852531	-0.051655	4.815541
247.108169	7999.975399	10.857536	-0.051649	4.815543
247.037939	7999.980681	10.862541	-0.051636	4.815545
247.145749	7999.882073	10.867546	-0.051657	4.815516
247.337787	7999.948240	10.872551	-0.051693	4.815534
247.258930	7999.962994	10.877555	-0.051678	4.815539
247.401264	7999.955727	10.882560	-0.051705	4.815536
247.481733	7999.966675	10.887565	-0.051720	4.815539
247.306659	7999.911506	10.892570	-0.051688	4.815524
247.313937	7999.927666	10.897575	-0.051689	4.815528
247.321365	7999.938489	10.902579	-0.051691	4.815532
247.304367	7999.914737	10.907584	-0.051688	4.815525
247.358440	7999.907097	10.912589	-0.051698	4.815522
247.129644	7999.931151	10.917594	-0.051656	4.815530
247.328721	7999.947238	10.922599	-0.051693	4.815534
247.087844	7999.897404	10.927603	-0.051649	4.815521
247.230376	7999.893344	10.932608	-0.051675	4.815519
247.306032	7999.946932	10.937613	-0.051690	4.815534
247.397874	7999.942045	10.942618	-0.051707	4.815532
247.358871	7999.977741	10.947623	-0.051700	4.815543
247.367571	7999.917029	10.952627	-0.051702	4.815525
247.422666	7999.916882	10.957632	-0.051712	4.815525
247.365549	7999.940535	10.962637	-0.051702	4.815532
247.168069	7999.917040	10.967642	-0.051666	4.815526
247.387579	7999.970841	10.972647	-0.051707	4.815541
247.433741	7999.895789	10.977651	-0.051716	4.815518
247.467213	7999.876065	10.982656	-0.051722	4.815513
247.581812	7999.955921	10.987661	-0.051744	4.815535
247.483686	7999.952204	10.992666	-0.051726	4.815535
247.372989	7999.977118	10.997671	-0.051705	4.815542
247.255544	7999.976289	11.002675	-0.051684	4.815543
247.521958	7999.960369	11.007680	-0.051733	4.815537
247.340054	7999.985188	11.012685	-0.051700	4.815545
247.048217	7999.944133	11.017690	-0.051646	4.815534
247.216737	7999.962925	11.022695	-0.051677	4.815539
247.173657	7999.928068	11.027699	-0.051670	4.815529
247.210714	7999.909471	11.032704	-0.051677	4.815523
247.271909	7999.947871	11.037709	-0.051688	4.815534
247.442847	7999.919711	11.042714	-0.051720	4.815525
247.505846	7999.974161	11.047719	-0.051732	4.815541
247.421058	7999.954642	11.052723	-0.051717	4.815536
247.486946	7999.917292	11.057728	-0.051729	4.815524
247.615763	7999.992040	11.062733	-0.051754	4.815546
247.404290	7999.932005	11.067738	-0.051714	4.815529
247.341735	7999.989744	11.072743	-0.051703	4.815546
247.343108	7999.964156	11.077747	-0.051704	4.815539
247.374787	7999.984987	11.082752	-0.051710	4.815545
247.294059	7999.965534	11.087757	-0.051695	4.815539
247.300585	7999.927215	11.092762	-0.051696	4.815528
247.340441	7999.977014	11.097767	-0.051704	4.815542
246.950916	7999.949316	11.102771	-0.051632	4.815536
247.161007	7999.939952	11.107776	-0.051671	4.815532
247.377343	7999.979817	11.112781	-0.051712	4.815543
247.120416	7999.964963	11.117786	-0.051664	4.815540
247.151911	7999.985791	11.122791	-0.051670	4.815546
247.338226	7999.950407	11.127795	-0.051705	4.815535
247.394432	7999.902218	11.132800	-0.051716	4.815520
247.222338	7999.983801	11.137805	-0.051684	4.815545
247.396943	7999.918322	11.142810	-0.051717	4.815525
247.491872	7999.974361	11.147815	-0.051735	4.815541
247.318913	7999.973694	11.152819	-0.051703	4.815542
247.308725	7999.950053	11.157824	-0.051701	4.815535
247.329263	7999.995265	11.162829	-0.051705	4.815548
247.277146	7999.982688	11.167834	-0.051696	4.815544
247.467353	8000.017855	11.172839	-0.051731	4.815554
247.293880	7999.939217	11.177843	-0.051699	4.815532
247.222804	7999.954097	11.182848	-0.051686	4.815536
247.432083	7999.982100	11.187853	-0.051726	4.815543
247.466366	7999.932485	11.192858	-0.051732	4.815529
247.525488	7999.964444	11.197863	-0.051743	4.815538
247.417198	7999.997941	11.202867	-0.051723	4.815548
247.534915	8000.018040	11.207872	-0.051746	4.815553
247.477880	8000.018198	11.212877	-0.051735	4.815554
247.205297	7999.969981	11.217882	-0.051685	4.815541
247.463175	8000.012661	11.222887	-0.051733	4.815552
247.609435	7999.954195	11.227891	-0.051760	4.815534
247.625313	7999.923504	11.232896	-0.051764	4.815525
247.512333	8000.009256	11.237901	-0.051743	4.815551
247.531183	7999.982885	11.242906	-0.051747	4.815543
247.669554	7999.955262	11.247911	-0.051773	4.815534
247.361445	7999.937437	11.252915	-0.051715	4.815531
247.502612	8000.001707	11.257920	-0.051742	4.815549
247.566932	8000.008118	11.262925	-0.051754	4.815550
247.519583	8000.018047	11.267930	-0.051746	4.815553
247.577077	8000.028619	11.272935	-0.051757	4.815556
247.607577	7999.989622	11.277939	-0.051763	4.815545
247.473965	7999.997074	11.282944	-0.051738	4.815547
247.497048	8000.018832	11.287949	-0.051743	4.815554
247.464675	7999.956381	11.292954	-0.051737	4.815536
247.647831	7999.932694	11.297959	-0.051771	4.815528
247.416932	7999.966324	11.302963	-0.051728	4.815539
247.558219	8000.018849	11.307968	-0.051755	4.815553
247.589355	8000.015107	11.312973	-0.051761	4.815552
247.488964	7999.947273	11.317978	-0.051742	4.815533
247.441023	7999.976415	11.322983	-0.051734	4.815542
247.446513	7999.942351	11.327987	-0.051735	4.815532
247.518977	7999.972391	11.332992	-0.051749	4.815540
247.419836	7999.988949	11.337997	-0.051731	4.815545
247.393227	7999.971448	11.343002	-0.051726	4.815540
247.421774	8000.011452	11.348007	-0.051731	4.815552
247.368346	7999.939045	11.353011	-0.051722	4.815531
247.523846	7999.965102	11.358016	-0.051751	4.815538
247.546147	7999.970827	11.363021	-0.051755	4.815539
247.522329	7999.904244	11.368026	-0.051751	4.815520
247.468921	7999.938637	11.373031	-0.051741	4.815530
247.459864	7999.936375	11.378035	-0.051740	4.815530
247.423176	7999.924049	11.383040	-0.051733	4.815526
247.581083	7999.951213	11.388045	-0.051763	4.815533
247.489401	7999.940125	11.393050	-0.051746	4.815531
247.594057	7999.979235	11.398055	-0.051766	4.815542
247.512195	7999.939472	11.403059	-0.051751	4.815530
247.571800	7999.915903	11.408064	-0.051762	4.815523
247.831305	7999.957542	11.413069	-0.051811	4.815534
247.656070	7999.970722	11.418074	-0.051778	4.815539
247.462778	8000.008170	11.423079	-0.051743	4.815551
247.371833	7999.958647	11.428083	-0.051726	4.815537
247.429668	7999.879514	11.433088	-0.051737	4.815513
247.581010	7999.888414	11.438093	-0.051765	4.815515
247.419319	7999.924243	11.443098	-0.051736	4.815526
247.934547	7999.965786	11.448103	-0.051832	4.815536
247.725926	7999.951720	11.453107	-0.051793	4.815533
247.666570	7999.881353	11.458112	-0.051782	4.815513
247.850603	7999.959139	11.463117	-0.051817	4.815534
247.578630	7999.923747	11.468122	-0.051766	4.815525
247.728891	7999.927290	11.473127	-0.051795	4.815526
247.615484	7999.917984	11.478131	-0.051774	4.815523
247.675415	7999.958500	11.483136	-0.051785	4.815535
247.486763	7999.935149	11.488141	-0.051750	4.815529
247.479080	7999.937181	11.493146	-0.051749	4.815530
247.621006	7999.956608	11.498151	-0.051776	4.815535
247.616556	7999.955488	11.503155	-0.051775	4.815534
247.603850	7999.917922	11.508160	-0.051773	4.815523
247.657631	7999.956202	11.513165	-0.051783	4.815534
247.603504	7999.956407	11.518170	-0.051774	4.815535
247.682027	7999.961983	11.523175	-0.051788	4.815536
247.343264	7999.884917	11.528179	-0.051725	4.815515
247.707485	7999.926130	11.533184	-0.051794	4.815525
247.664533	7999.982054	11.538189	-0.051786	4.815542
247.576545	7999.941122	11.543194	-0.051770	4.815530
247.775281	7999.994585	11.548199	-0.051807	4.815545
247.598699	7999.958615	11.553203	-0.051774	4.815535
247.598193	7999.930860	11.558208	-0.051774	4.815527
247.461898	7999.978851	11.563213	-0.051749	4.815542
247.623966	7999.917440	11.568218	-0.051780	4.815523
247.628999	8000.013663	11.573223	-0.051781	4.815551
247.668047	7999.950242	11.578227	-0.051788	4.815532
247.556777	7999.914271	11.583232	-0.051768	4.815523
247.528402	7999.952276	11.588237	-0.051763	4.815534
247.533206	7999.949172	11.593242	-0.051764	4.815533
247.611115	7999.965418	11.598247	-0.051779	4.815537
247.544979	7999.946203	11.603251	-0.051767	4.815532
247.568956	7999.907101	11.608256	-0.051771	4.815520
247.786258	7999.933099	11.613261	-0.051812	4.815527
247.470466	7999.909807	11.618266	-0.051754	4.815522
247.598744	7999.966391	11.623271	-0.051778	4.815537
247.550534	7999.982713	11.628275	-0.051769	4.815542
247.723604	7999.958861	11.633280	-0.051801	4.815535
247.685382	7999.973210	11.638285	-0.051795	4.815539
247.555558	7999.983927	11.643290	-0.051771	4.815543
247.613318	7999.978484	11.648295	-0.051782	4.815541
247.655782	7999.941819	11.653299	-0.051790	4.815530
247.627785	7999.969151	11.658304	-0.051785	4.815538
247.524741	7999.955742	11.663309	-0.051766	4.815535
247.783830	7999.929022	11.668314	-0.051814	4.815526
247.613393	7999.963640	11.673319	-0.051783	4.815537
247.561048	7999.971351	11.678323	-0.051773	4.815539
247.611210	7999.905976	11.683328	-0.051783	4.815520
247.777956	7999.952508	11.688333	-0.051814	4.815532
247.493413	7999.945747	11.693338	-0.051762	4.815532
247.634550	8000.003609	11.698343	-0.051788	4.815548
247.595052	7999.955993	11.703347	-0.051781	4.815534
247.688002	7999.993844	11.708352	-0.051799	4.815545
247.628576	8000.011051	11.713357	-0.051788	4.815550
247.617026	8000.047196	11.718362	-0.051786	4.815561
247.691331	8000.052703	11.723367	-0.051800	4.815562
247.487718	8000.000271	11.728371	-0.051762	4.815548
247.529422	7999.963594	11.733376	-0.051770	4.815537
247.782884	7999.980570	11.738381	-0.051818	4.815541
247.506615	7999.967536	11.743386	-0.051766	4.815538
247.566235	7999.999503	11.748391	-0.051778	4.815547
247.448165	7999.937789	11.753395	-0.051756	4.815530
247.231748	7999.905441	11.758400	-0.051716	4.815521
247.388708	7999.985988	11.763405	-0.051745	4.815544
247.448129	7999.895133	11.768410	-0.051757	4.815517
247.536865	7999.961750	11.773415	-0.051774	4.815536
247.501458	7999.972942	11.778419	-0.051767	4.815540
247.483003	7999.968390	11.783424	-0.051764	4.815538
247.790610	7999.994795	11.788429	-0.051822	4.815545
247.586820	7999.887892	11.793434	-0.051784	4.815514
247.780803	7999.914577	11.798439	-0.051820	4.815521
247.914280	7999.990471	11.803443	-0.051845	4.815543
247.747375	7999.966406	11.808448	-0.051814	4.815537
247.569053	7999.985943	11.813453	-0.051782	4.815543
247.650210	7999.972338	11.818458	-0.051797	4.815539
247.677215	7999.981344	11.823463	-0.051802	4.815541
247.610741	7999.931152	11.828467	-0.051790	4.815527
247.638158	7999.897446	11.833472	-0.051795	4.815517
247.855142	7999.961887	11.838477	-0.051836	4.815535
247.662224	7999.877590	11.843482	-0.051800	4.815511
247.673567	7999.922652	11.848487	-0.051803	4.815524
247.730735	7999.928947	11.853491	-0.051814	4.815526
247.804531	7999.900270	11.858496	-0.051827	4.815517
247.672412	7999.922697	11.863501	-0.051803	4.815524
247.394138	7999.861571	11.868506	-0.051752	4.815508
247.617476	7999.891939	11.873511	-0.051793	4.815515
247.414619	7999.907872	11.878515	-0.051756	4.815521
247.481301	7999.950634	11.883520	-0.051769	4.815533
247.408686	7999.963353	11.888525	-0.051755	4.815537
247.325982	7999.939596	11.893530	-0.051740	4.815531
247.447318	7999.951211	11.898535	-0.051763	4.815533
247.557449	7999.930603	11.903539	-0.051784	4.815527
247.424750	7999.901758	11.908544	-0.051759	4.815519
247.435109	7999.958552	11.913549	-0.051761	4.815536
247.352064	7999.889934	11.918554	-0.051746	4.815516
247.559082	7999.942463	11.923559	-0.051785	4.815530
247.390898	7999.954690	11.928563	-0.051754	4.815535
247.415761	7999.856863	11.933568	-0.051759	4.815506
247.567400	7999.930915	11.938573	-0.051787	4.815527
247.553283	7999.869831	11.943578	-0.051785	4.815509
247.571642	7999.938503	11.948583	-0.051789	4.815529
247.644533	7999.914083	11.953587	-0.051802	4.815522
247.647084	7999.881039	11.958592	-0.051803	4.815512
247.639322	7999.942877	11.963597	-0.051802	4.815530
247.548407	7999.929666	11.968602	-0.051785	4.815527
247.724521	7999.919747	11.973607	-0.051818	4.815523
247.693462	7999.886153	11.978611	-0.051813	4.815513
247.799027	7999.837703	11.983616	-0.051833	4.815498
247.965792	7999.938704	11.988621	-0.051864	4.815527
247.543711	7999.893384	11.993626	-0.051786	4.815516
247.526301	7999.852538	11.998631	-0.051782	4.815504
247.623465	7999.921429	12.003635	-0.051801	4.815524
247.616331	7999.915994	12.008640	-0.051800	4.815522
247.647498	7999.978468	12.013645	-0.051806	4.815540
247.684846	7999.921428	12.018650	-0.051813	4.815523
247.676616	7999.922383	12.023655	-0.051812	4.815524
247.620708	7999.900131	12.028659	-0.051802	4.815518
247.616778	7999.900088	12.033664	-0.051801	4.815518
247.683781	7999.940720	12.038669	-0.051814	4.815529
247.547924	7999.878715	12.043674	-0.051789	4.815512
247.783051	7999.946656	12.048679	-0.051833	4.815530
247.729785	7999.970372	12.053683	-0.051823	4.815537
247.695126	7999.887591	12.058688	-0.051817	4.815513
247.520913	7999.953119	12.063693	-0.051785	4.815533
247.227466	7999.892813	12.068698	-0.051730	4.815517
247.565068	7999.934659	12.073703	-0.051793	4.815528
247.737046	7999.938557	12.078707	-0.051826	4.815528
247.371375	7999.906975	12.083712	-0.051758	4.815521
247.630944	7999.915507	12.088717	-0.051806	4.815522
247.601464	7999.894755	12.093722	-0.051801	4.815516
247.461812	7999.928808	12.098727	-0.051775	4.815527
247.597938	7999.906488	12.103731	-0.051801	4.815519
247.713226	7999.887033	12.108736	-0.051823	4.815513
247.594378	7999.972689	12.113741	-0.051801	4.815539
247.671378	7999.949404	12.118746	-0.051815	4.815532
247.835837	7999.930751	12.123751	-0.051846	4.815525
247.700331	7999.880500	12.128755	-0.051821	4.815511
247.449432	7999.879628	12.133760	-0.051775	4.815512
247.743424	7999.941054	12.138765	-0.051830	4.815529
247.718559	7999.881929	12.143770	-0.051825	4.815512
247.637816	7999.941508	12.148775	-0.051811	4.815529
247.575886	7999.947994	12.153779	-0.051799	4.815532
247.624525	7999.891138	12.158784	-0.051809	4.815515
247.643514	7999.974773	12.163789	-0.051812	4.815539
247.634977	7999.936207	12.168794	-0.051811	4.815528
247.785721	7999.966459	12.173799	-0.051839	4.815536
247.776607	7999.920407	12.178803	-0.051838	4.815523
247.584644	7999.915158	12.183808	-0.051802	4.815522
247.805846	7999.979668	12.188813	-0.051844	4.815540
247.539419	7999.924074	12.193818	-0.051794	4.815525
247.603070	7999.919795	12.198823	-0.051807	4.815523
247.545429	7999.921011	12.203827	-0.051796	4.815524
247.682744	7999.858127	12.208832	-0.051822	4.815505
247.679424	7999.893338	12.213837	-0.051822	4.815515
247.580530	7999.869316	12.218842	-0.051803	4.815508
247.801175	7999.913525	12.223847	-0.051845	4.815520
247.803749	7999.903976	12.228851	-0.051845	4.815518
247.801922	7999.894356	12.233856	-0.051845	4.815515
247.782959	7999.960284	12.238861	-0.051842	4.815534
247.819316	7999.917111	12.243866	-0.051849	4.815521
247.829277	7999.922635	12.248871	-0.051851	4.815523
247.684293	7999.975825	12.253875	-0.051824	4.815539
247.576488	7999.915345	12.258880	-0.051805	4.815522
247.806511	7999.974660	12.263885	-0.051848	4.815538
247.626767	7999.996309	12.268890	-0.051814	4.815545
247.805357	7999.989636	12.273895	-0.051848	4.815542
247.681389	7999.966272	12.278899	-0.051825	4.815536
247.768018	7999.931396	12.283904	-0.051841	4.815526
247.812028	7999.924661	12.288909	-0.051850	4.815523
247.647729	7999.942291	12.293914	-0.051820	4.815529
247.723254	7999.988402	12.298919	-0.051834	4.815542
247.609779	7999.931034	12.303923	-0.051813	4.815526
247.753154	7999.858637	12.308928	-0.051840	4.815504
247.808990	7999.901222	12.313933	-0.051851	4.815517
247.545603	7999.912962	12.318938	-0.051802	4.815521
247.710717	7999.931700	12.323943	-0.051833	4.815526
247.713060	7999.936031	12.328947	-0.051833	4.815527
247.661911	7999.908517	12.333952	-0.051824	4.815519
247.708096	7999.916769	12.338957	-0.051833	4.815522
247.698144	7999.930512	12.343962	-0.051831	4.815526
247.824517	7999.962502	12.348967	-0.051855	4.815534
247.710677	7999.972412	12.353971	-0.051834	4.815538
247.704913	7999.987291	12.358976	-0.051833	4.815542
247.884469	8000.004129	12.363981	-0.051867	4.815546
247.643454	7999.933998	12.368986	-0.051822	4.815527
247.727530	7999.924712	12.373991	-0.051838	4.815524
247.630979	7999.972285	12.378995	-0.051821	4.815538
247.798268	7999.916298	12.384000	-0.051852	4.815521
247.757352	7999.929536	12.389005	-0.051845	4.815525
247.550796	7999.826860	12.394010	-0.051806	4.815496
247.811297	7999.890943	12.399015	-0.051855	4.815513
247.643207	7999.921328	12.404019	-0.051824	4.815523
247.655762	7999.904466	12.409024	-0.051827	4.815518
247.899998	7999.967217	12.414029	-0.051872	4.815535
247.700688	7999.815531	12.419034	-0.051835	4.815492
247.896336	7999.778163	12.424039	-0.051872	4.815480
247.996588	7999.825746	12.429043	-0.051891	4.815493
247.878420	7999.814225	12.434048	-0.051869	4.815491
247.916735	7999.847981	12.439053	-0.051877	4.815500
247.805432	7999.888904	12.444058	-0.051856	4.815513
248.002128	7999.986123	12.449063	-0.051893	4.815540
247.796920	7999.940072	12.454067	-0.051855	4.815528
247.796856	7999.876012	12.459072	-0.051855	4.815509
248.117438	7999.922922	12.464077	-0.051915	4.815521
248.114405	7999.883378	12.469082	-0.051915	4.815510
247.942490	7999.928651	12.474087	-0.051883	4.815524
247.995119	7999.922056	12.479091	-0.051893	4.815522
247.940764	7999.897694	12.484096	-0.051883	4.815515
248.119744	7999.989284	12.489101	-0.051917	4.815541
248.037661	7999.930291	12.494106	-0.051902	4.815524
248.079796	7999.905369	12.499111	-0.051910	4.815516
247.859578	7999.926357	12.504115	-0.051869	4.815523
247.770976	7999.881144	12.509120	-0.051853	4.815511
247.939369	7999.958676	12.514125	-0.051885	4.815532
247.845703	7999.952895	12.519130	-0.051867	4.815531
247.856892	7999.937079	12.524135	-0.051870	4.815527
247.965246	7999.937803	12.529139	-0.051890	4.815526
248.220013	7999.925965	12.534144	-0.051938	4.815522
248.116808	7999.965953	12.539149	-0.051919	4.815534
248.106033	7999.930554	12.544154	-0.051917	4.815523
248.075708	7999.971733	12.549159	-0.051912	4.815536
247.872989	7999.955627	12.554163	-0.051874	4.815532
247.786621	7999.878409	12.559168	-0.051858	4.815510
247.791168	7999.963945	12.564173	-0.051859	4.815535
248.007676	7999.932259	12.569178	-0.051900	4.815524
247.846288	7999.911488	12.574183	-0.051870	4.815519
247.803037	7999.925755	12.579187	-0.051862	4.815523
247.758898	7999.916512	12.584192	-0.051854	4.815521
248.050229	7999.929835	12.589197	-0.051909	4.815523
247.869275	7999.900201	12.594202	-0.051875	4.815516
248.190646	7999.908676	12.599207	-0.051936	4.815517
248.011991	7999.970928	12.604211	-0.051903	4.815536
247.788457	8000.040990	12.609216	-0.051861	4.815557
247.801772	7999.986761	12.614221	-0.051864	4.815541
247.787782	7999.979077	12.619226	-0.051862	4.815539
247.840471	7999.962871	12.624231	-0.051872	4.815534
247.798548	7999.971820	12.629235	-0.051864	4.815537
247.762822	7999.901838	12.634240	-0.051858	4.815517
247.877683	7999.891987	12.639245	-0.051879	4.815513
247.821932	7999.899642	12.644250	-0.051869	4.815516
247.837515	7999.908462	12.649255	-0.051872	4.815518
248.007064	7999.947565	12.654259	-0.051904	4.815529
247.921258	7999.964341	12.659264	-0.051888	4.815534
247.910917	7999.999438	12.664269	-0.051887	4.815544
247.990738	7999.933478	12.669274	-0.051902	4.815525
247.811166	7999.920954	12.674279	-0.051869	4.815522
247.727889	7999.940976	12.679283	-0.051853	4.815528
247.996560	7999.909073	12.684288	-0.051904	4.815518
247.952840	7999.922265	12.689293	-0.051896	4.815522
247.864231	7999.916567	12.694298	-0.051879	4.815520
247.862210	7999.955003	12.699303	-0.051879	4.815532
247.873837	7999.948807	12.704307	-0.051882	4.815530
247.736257	7999.869685	12.709312	-0.051856	4.815507
247.850606	7999.961286	12.714317	-0.051878	4.815533
247.918354	7999.871634	12.719322	-0.051891	4.815507
247.864227	7999.886791	12.724327	-0.051881	4.815512
247.804030	7999.869809	12.729331	-0.051870	4.815507
248.065934	7999.839932	12.734336	-0.051919	4.815497
248.101640	7999.952678	12.739341	-0.051926	4.815530
247.878970	7999.933042	12.744346	-0.051885	4.815525
247.961613	7999.944025	12.749351	-0.051900	4.815528
247.992967	7999.953103	12.754355	-0.051906	4.815530
247.782946	7999.859981	12.759360	-0.051867	4.815504
248.017366	7999.920436	12.764365	-0.051911	4.815521
248.157350	7999.933424	12.769370	-0.051938	4.815524
248.244492	7999.946617	12.774375	-0.051954	4.815527
247.929422	7999.948968	12.779379	-0.051896	4.815529
247.956928	7999.912058	12.784384	-0.051901	4.815518
248.027928	7999.970912	12.789389	-0.051915	4.815535
247.811156	7999.920400	12.794394	-0.051874	4.815522
247.998493	7999.944842	12.799399	-0.051910	4.815528
247.984372	7999.952108	12.804403	-0.051907	4.815530
247.957999	7999.889754	12.809408	-0.051902	4.815512
248.031189	7999.959324	12.814413	-0.051916	4.815532
247.973443	7999.885777	12.819418	-0.051906	4.815511
247.970138	7999.864385	12.824423	-0.051905	4.815504
247.959105	7999.902674	12.829427	-0.051904	4.815516
248.020038	7999.941071	12.834432	-0.051915	4.815527
248.065021	7999.933283	12.839437	-0.051924	4.815524
247.850315	7999.868921	12.844442	-0.051884	4.815506
248.157603	7999.903866	12.849447	-0.051942	4.815515
248.120658	7999.942801	12.854451	-0.051935	4.815527
247.925232	7999.878753	12.859456	-0.051899	4.815509
248.146404	7999.951808	12.864461	-0.051940	4.815529
248.124342	7999.892728	12.869466	-0.051936	4.815512
248.190713	7999.911990	12.874471	-0.051949	4.815517
248.016496	7999.911302	12.879475	-0.051917	4.815518
248.068096	7999.847017	12.884480	-0.051927	4.815499
248.062950	7999.939872	12.889485	-0.051926	4.815526
247.842847	7999.882897	12.894490	-0.051885	4.815510
248.052852	7999.928001	12.899495	-0.051924	4.815523
247.985058	7999.970704	12.904499	-0.051912	4.815535
247.872208	7999.899461	12.909504	-0.051891	4.815515
247.890362	7999.937159	12.914509	-0.051895	4.815526
247.903767	7999.842347	12.919514	-0.051898	4.815498
247.947272	7999.875119	12.924519	-0.051906	4.815508
248.024039	7999.918047	12.929523	-0.051921	4.815520
248.148664	7999.925444	12.934528	-0.051944	4.815521
248.135663	7999.867581	12.939533	-0.051942	4.815504
247.952898	7999.898793	12.944538	-0.051908	4.815514
248.235303	7999.962169	12.949543	-0.051961	4.815532
248.311902	7999.948489	12.954547	-0.051975	4.815527
248.090647	7999.943828	12.959552	-0.051934	4.815527
247.867143	8000.005347	12.964557	-0.051893	4.815546
247.946084	7999.928693	12.969562	-0.051908	4.815523
248.089238	7999.926781	12.974567	-0.051935	4.815522
247.993290	7999.922031	12.979571	-0.051917	4.815521
247.620718	7999.841207	12.984576	-0.051848	4.815499
247.967755	7999.979329	12.989581	-0.051913	4.815538
247.860620	7999.974397	12.994586	-0.051893	4.815537
247.891670	7999.980265	12.999591	-0.051899	4.815538
247.830377	7999.969673	13.004595	-0.051888	4.815536
247.935564	7999.909468	13.009600	-0.051908	4.815518
247.927296	7999.913627	13.014605	-0.051907	4.815519
247.934331	7999.924443	13.019610	-0.051908	4.815522
248.022880	7999.977176	13.024615	-0.051925	4.815537
247.979194	7999.876090	13.029619	-0.051917	4.815508
247.971851	7999.893080	13.034624	-0.051916	4.815513
248.307982	7999.958401	13.039629	-0.051979	4.815530
248.198505	7999.919253	13.044634	-0.051959	4.815519
248.047622	7999.958463	13.049639	-0.051931	4.815531
248.012847	7999.938692	13.054643	-0.051925	4.815526
248.022333	7999.907896	13.059648	-0.051927	4.815517
248.074797	7999.903434	13.064653	-0.051937	4.815515
247.957521	7999.936784	13.069658	-0.051915	4.815525
247.973684	7999.952022	13.074663	-0.051918	4.815530
248.036590	7999.935982	13.079667	-0.051930	4.815525
248.006174	7999.875698	13.084672	-0.051925	4.815507
248.234532	7999.969163	13.089677	-0.051968	4.815533
248.111765	7999.924459	13.094682	-0.051945	4.815521
248.213850	7999.919740	13.099687	-0.051964	4.815519
248.273530	7999.972001	13.104691	-0.051976	4.815534
248.180433	7999.945937	13.109696	-0.051959	4.815527
248.074481	7999.969860	13.114701	-0.051939	4.815534
248.245524	7999.941703	13.119706	-0.051971	4.815525
248.089136	7999.944510	13.124711	-0.051942	4.815527
248.020353	7999.925251	13.129715	-0.051930	4.815522
248.088322	7999.937063	13.134720	-0.051943	4.815525
248.129930	7999.928152	13.139725	-0.051951	4.815522
248.047892	7999.953534	13.144730	-0.051936	4.815530
247.981546	7999.971695	13.149735	-0.051923	4.815535
247.794886	7999.948375	13.154739	-0.051889	4.815529
248.046992	7999.858530	13.159744	-0.051936	4.815502
247.970171	7999.927785	13.164749	-0.051922	4.815523
248.215365	7999.874139	13.169754	-0.051968	4.815506
248.104335	7999.949244	13.174759	-0.051948	4.815528
248.091581	8000.015274	13.179763	-0.051945	4.815547
247.790975	7999.912128	13.184768	-0.051890	4.815519
247.869206	7999.933719	13.189773	-0.051904	4.815525
248.000957	7999.926281	13.194778	-0.051929	4.815522
247.821104	7999.941520	13.199783	-0.051896	4.815527
248.056579	7999.962477	13.204787	-0.051940	4.815532
248.060755	7999.899553	13.209792	-0.051941	4.815514
248.060781	7999.936956	13.214797	-0.051941	4.815525
247.745737	7999.961735	13.219802	-0.051883	4.815533
248.028441	7999.977055	13.224807	-0.051936	4.815537
248.056258	7999.993551	13.229811	-0.051941	4.815541
247.947574	7999.907424	13.234816	-0.051921	4.815517
248.228920	7999.973986	13.239821	-0.051974	4.815535
248.272002	7999.910630	13.244826	-0.051982	4.815516
247.944395	7999.894620	13.249831	-0.051921	4.815513
248.180185	7999.893153	13.254835	-0.051966	4.815511
248.232451	7999.892960	13.259840	-0.051975	4.815511
248.043410	7999.958246	13.264845	-0.051941	4.815531
247.697948	7999.916312	13.269850	-0.051876	4.815520
247.994754	7999.959630	13.274855	-0.051932	4.815532
248.096401	7999.945292	13.279859	-0.051951	4.815527
247.933565	7999.934109	13.284864	-0.051921	4.815524
247.910133	8000.011713	13.289869	-0.051917	4.815547
248.181416	7999.937133	13.294874	-0.051968	4.815524
248.233169	7999.963632	13.299879	-0.051978	4.815532
248.125510	7999.936262	13.304883	-0.051958	4.815524
248.090825	7999.846004	13.309888	-0.051952	4.815498
248.246561	7999.887018	13.314893	-0.051981	4.815509
248.067292	7999.892655	13.319898	-0.051948	4.815512
248.013056	7999.931307	13.324903	-0.051938	4.815523
248.060162	7999.968410	13.329907	-0.051947	4.815534
248.033653	7999.869741	13.334912	-0.051942	4.815505
248.079834	7999.923918	13.339917	-0.051951	4.815521
248.126202	7999.872364	13.344922	-0.051960	4.815505
248.169194	7999.886972	13.349927	-0.051968	4.815509
248.031683	7999.953100	13.354931	-0.051943	4.815529
248.232690	7999.896596	13.359936	-0.051980	4.815512
248.119883	8000.000509	13.364941	-0.051960	4.815543
247.896794	7999.921056	13.369946	-0.051918	4.815521
248.033780	7999.937200	13.374951	-0.051944	4.815525
248.270614	7999.966723	13.379955	-0.051988	4.815532
248.166937	7999.872133	13.384960	-0.051969	4.815505
248.277068	7999.933762	13.389965	-0.051990	4.815523
248.125250	7999.963344	13.394970	-0.051962	4.815532
248.217473	7999.931763	13.399975	-0.051980	4.815522
248.070965	7999.956092	13.404979	-0.051953	4.815530
247.942985	7999.911302	13.409984	-0.051929	4.815518
248.178087	7999.986721	13.414989	-0.051973	4.815538
248.180414	7999.898135	13.419994	-0.051974	4.815513
248.155601	7999.973580	13.424999	-0.051969	4.815535
248.286064	7999.944761	13.430003	-0.051994	4.815526
248.280801	7999.764201	13.435008	-0.051993	4.815473
248.541875	7999.821888	13.440013	-0.052042	4.815488
248.259660	7999.876040	13.445018	-0.051990	4.815506
248.437734	7999.904603	13.450023	-0.052023	4.815513
248.389842	7999.964720	13.455027	-0.052014	4.815531
248.487069	7999.843507	13.460032	-0.052033	4.815495
248.551180	7999.924678	13.465037	-0.052045	4.815518
248.342915	7999.951201	13.470042	-0.052006	4.815527
248.421235	7999.954638	13.475047	-0.052021	4.815528
248.535502	7999.965071	13.480051	-0.052043	4.815530
248.536455	7999.954428	13.485056	-0.052043	4.815527
248.328299	8000.009789	13.490061	-0.052005	4.815544
248.436330	7999.922930	13.495066	-0.052025	4.815518
248.535065	7999.961945	13.500071	-0.052044	4.815529
248.535125	8000.019641	13.505075	-0.052044	4.815546
248.437234	7999.933689	13.510080	-0.052026	4.815522
248.645491	7999.939249	13.515085	-0.052065	4.815522
248.401380	7999.952370	13.520090	-0.052020	4.815527
248.365692	7999.931516	13.525095	-0.052013	4.815521
248.476269	7999.955773	13.530099	-0.052034	4.815528
248.241484	7999.856904	13.535104	-0.051991	4.815500
248.457930	7999.918135	13.540109	-0.052031	4.815517
248.415269	7999.913187	13.545114	-0.052023	4.815516
248.422316	7999.898372	13.550119	-0.052025	4.815511
248.279861	7999.917426	13.555123	-0.051999	4.815518
248.346306	7999.907853	13.560128	-0.052011	4.815514
248.608843	7999.951681	13.565133	-0.052060	4.815526
248.480239	7999.935716	13.570138	-0.052037	4.815522
248.296157	7999.976519	13.575143	-0.052003	4.815535
248.328610	7999.985615	13.580147	-0.052009	4.815537
248.557997	7999.919963	13.585152	-0.052052	4.815517
248.489862	7999.917803	13.590157	-0.052040	4.815517
248.449900	7999.853090	13.595162	-0.052032	4.815498
248.538291	7999.846011	13.600167	-0.052049	4.815495
248.564259	7999.889178	13.605171	-0.052054	4.815508
248.353172	7999.928471	13.610176	-0.052015	4.815520
248.420639	7999.911439	13.615181	-0.052028	4.815515
248.571884	7999.903251	13.620186	-0.052056	4.815512
248.414871	7999.904979	13.625191	-0.052027	4.815513
248.461703	7999.960235	13.630195	-0.052036	4.815529
248.308743	7999.874452	13.635200	-0.052008	4.815505
248.328001	7999.955957	13.640205	-0.052012	4.815528
248.241214	7999.953493	13.645210	-0.051996	4.815528
248.620869	7999.889228	13.650215	-0.052067	4.815508
248.380460	7999.937654	13.655219	-0.052022	4.815523
248.306895	7999.862780	13.660224	-0.052009	4.815501
248.552101	7999.955454	13.665229	-0.052055	4.815527
248.509253	7999.876809	13.670234	-0.052047	4.815504
248.271023	7999.886823	13.675239	-0.052003	4.815508
248.371948	7999.973935	13.680243	-0.052022	4.815533
248.586825	7999.981740	13.685248	-0.052062	4.815535
248.474896	7999.961776	13.690253	-0.052042	4.815529
248.240071	7999.941940	13.695258	-0.051998	4.815525
248.340022	7999.940390	13.700263	-0.052017	4.815524
248.403983	7999.952137	13.705267	-0.052029	4.815527
248.449228	7999.906973	13.710272	-0.052038	4.815513
248.500394	7999.974048	13.715277	-0.052048	4.815533
248.520101	7999.904969	13.720282	-0.052052	4.815513
248.569841	7999.915416	13.725287	-0.052061	4.815515
248.466557	7999.940450	13.730291	-0.052042	4.815523
248.375201	7999.926163	13.735296	-0.052025	4.815519
248.474995	7999.902182	13.740301	-0.052044	4.815512
248.434285	7999.923967	13.745306	-0.052037	4.815518
248.374002	7999.939024	13.750311	-0.052026	4.815523
248.471431	7999.939569	13.755315	-0.052044	4.815523
248.573235	7999.887852	13.760320	-0.052063	4.815507
248.711823	7999.902955	13.765325	-0.052089	4.815511
248.605096	7999.886280	13.770330	-0.052070	4.815507
248.549536	7999.906754	13.775335	-0.052060	4.815513
248.629313	7999.958276	13.780339	-0.052075	4.815528
248.369675	7999.946579	13.785344	-0.052027	4.815525
248.485169	7999.958100	13.790349	-0.052048	4.815528
248.249296	7999.900866	13.795354	-0.052005	4.815513
248.404504	7999.875654	13.800359	-0.052034	4.815504
248.529994	7999.950352	13.805363	-0.052058	4.815526
248.469972	7999.875699	13.810368	-0.052047	4.815504
248.593292	7999.949293	13.815373	-0.052070	4.815525
248.582558	7999.969432	13.820378	-0.052068	4.815531
248.649793	7999.906470	13.825383	-0.052081	4.815512
248.576801	7999.937340	13.830387	-0.052067	4.815522
248.426700	7999.932772	13.835392	-0.052040	4.815521
248.589232	7999.955742	13.840397	-0.052070	4.815527
248.434322	7999.910511	13.845402	-0.052042	4.815514
248.581833	7999.936440	13.850407	-0.052069	4.815521
248.523731	7999.949396	13.855411	-0.052059	4.815525
248.437131	7999.893533	13.860416	-0.052043	4.815509
248.728982	7999.967745	13.865421	-0.052098	4.815530
248.683886	7999.947805	13.870426	-0.052089	4.815524
248.501274	7999.897849	13.875431	-0.052056	4.815510
248.455081	7999.944109	13.880435	-0.052047	4.815524
248.640461	7999.861717	13.885440	-0.052082	4.815499
248.659730	7999.940020	13.890445	-0.052086	4.815522
248.264191	7999.916490	13.895450	-0.052012	4.815517
248.390373	7999.935661	13.900455	-0.052036	4.815522
248.495291	7999.974778	13.905459	-0.052056	4.815533
248.503445	7999.950368	13.910464	-0.052058	4.815526
248.503680	7999.935441	13.915469	-0.052058	4.815521
248.455930	7999.917594	13.920474	-0.052049	4.815516
248.459762	7999.967875	13.925479	-0.052050	4.815531
248.515179	7999.995503	13.930483	-0.052061	4.815539
248.475943	7999.932937	13.935488	-0.052054	4.815521
248.463230	7999.964792	13.940493	-0.052052	4.815530
248.543047	7999.944757	13.945498	-0.052067	4.815524
248.501375	7999.904580	13.950503	-0.052059	4.815512
248.429468	7999.992073	13.955507	-0.052046	4.815538
248.320930	7999.931579	13.960512	-0.052026	4.815521
248.440622	7999.911128	13.965517	-0.052049	4.815514
248.502020	7999.914289	13.970522	-0.052060	4.815515
248.486552	7999.894833	13.975527	-0.052058	4.815509
248.453895	7999.935974	13.980531	-0.052052	4.815522
248.676807	7999.886236	13.985536	-0.052094	4.815506
248.714829	7999.883675	13.990541	-0.052101	4.815505
248.554576	7999.943023	13.995546	-0.052071	4.815523
248.595225	7999.930893	14.000551	-0.052079	4.815519
248.747888	7999.936613	14.005555	-0.052108	4.815520
248.801913	7999.927905	14.010560	-0.052118	4.815518
248.661737	7999.939520	14.015565	-0.052092	4.815522
248.778675	7999.867758	14.020570	-0.052114	4.815500
248.651478	7999.883857	14.025575	-0.052091	4.815505
248.612556	7999.918488	14.030579	-0.052084	4.815516
248.648344	7999.918026	14.035584	-0.052091	4.815515
248.606190	7999.970760	14.040589	-0.052083	4.815531
248.544510	7999.958025	14.045594	-0.052072	4.815528
248.524230	7999.891497	14.050599	-0.052068	4.815508
248.600612	7999.932284	14.055603	-0.052083	4.815520
248.605963	7999.892876	14.060608	-0.052084	4.815508
248.532024	7999.962179	14.065613	-0.052071	4.815529
248.576861	7999.928756	14.070618	-0.052079	4.815519
248.798272	7999.955893	14.075623	-0.052121	4.815526
248.727787	7999.973987	14.080627	-0.052108	4.815531
248.727603	7999.929148	14.085632	-0.052108	4.815518
248.771145	7999.921336	14.090637	-0.052116	4.815516
248.733728	7999.915406	14.095642	-0.052110	4.815514
248.781290	7999.934361	14.100647	-0.052119	4.815519
248.742762	7999.976475	14.105651	-0.052112	4.815532
248.880919	7999.972346	14.110656	-0.052138	4.815530
248.764814	7999.970470	14.115661	-0.052116	4.815530
248.855724	7999.992270	14.120666	-0.052134	4.815536
248.968733	7999.935396	14.125671	-0.052155	4.815519
248.815567	7999.983112	14.130675	-0.052127	4.815533
248.538535	7999.963653	14.135680	-0.052075	4.815529
248.614262	8000.019382	14.140685	-0.052090	4.815545
248.644369	7999.987855	14.145690	-0.052095	4.815536
248.594071	7999.972101	14.150695	-0.052086	4.815531
248.638126	7999.974979	14.155699	-0.052095	4.815532
248.616793	7999.879597	14.160704	-0.052091	4.815504
248.675474	7999.955339	14.165709	-0.052102	4.815526
248.846273	7999.929315	14.170714	-0.052134	4.815518
248.965921	7999.914203	14.175719	-0.052157	4.815513
248.913444	7999.966769	14.180723	-0.052147	4.815528
248.519915	7999.893073	14.185728	-0.052074	4.815508
248.870181	8000.006691	14.190733	-0.052140	4.815540
248.921062	7999.990455	14.195738	-0.052149	4.815535
248.959619	7999.894983	14.200743	-0.052157	4.815507
248.874000	7999.948075	14.205747	-0.052141	4.815523
248.649792	7999.896370	14.210752	-0.052100	4.815509
248.737693	7999.946958	14.215757	-0.052116	4.815523
248.603842	7999.925567	14.220762	-0.052092	4.815518
248.902470	7999.957170	14.225767	-0.052147	4.815525
248.976203	8000.021412	14.230771	-0.052161	4.815544
248.797113	7999.938402	14.235776	-0.052128	4.815520
249.004838	7999.975996	14.240781	-0.052167	4.815530
248.741492	7999.961033	14.245786	-0.052118	4.815527
248.778336	7999.980881	14.250791	-0.052125	4.815533
248.883564	7999.983691	14.255795	-0.052145	4.815533
248.715839	7999.662698	14.260800	-0.052114	4.815440

248.843507	7996.435417	14.265805	-0.052136	4.814496
248.971529	7990.794005	14.270810	-0.052156	4.812846
248.926753	7983.983323	14.275815	-0.052144	4.810854
248.764461	7976.690482	14.280819	-0.052109	4.808720
248.430501	7969.020887	14.285824	-0.052042	4.806476
248.747100	7961.208395	14.290829	-0.052096	4.804186
248.613533	7953.395864	14.295834	-0.052067	4.801897
248.615942	7945.386905	14.300839	-0.052062	4.799548
248.530466	7937.427385	14.305843	-0.052041	4.797214
248.359729	7929.366315	14.310848	-0.052004	4.794849
248.489561	7921.441186	14.315853	-0.052024	4.792521
248.308114	7913.318889	14.320858	-0.051985	4.790135
248.555627	7905.439292	14.325863	-0.052026	4.787818
248.302553	7897.377117	14.330867	-0.051974	4.785448
248.330689	7889.427905	14.335872	-0.051974	4.783109
248.267172	7881.421966	14.340877	-0.051957	4.780753
248.307464	7873.412908	14.345882	-0.051960	4.778394
248.202705	7865.446151	14.350887	-0.051936	4.776047
248.012961	7857.403918	14.355891	-0.051895	4.773676
248.018708	7849.347078	14.360896	-0.051891	4.771300
248.078200	7841.293872	14.365901	-0.051897	4.768923
247.889744	7833.400185	14.370906	-0.051857	4.766593
248.049600	7825.340316	14.375911	-0.051882	4.764212
247.935849	7817.450136	14.380915	-0.051856	4.761880
247.717010	7809.307193	14.385920	-0.051810	4.759473
247.775929	7801.380560	14.390925	-0.051816	4.757128
247.817289	7793.373261	14.395930	-0.051819	4.754758
247.693301	7785.309083	14.400935	-0.051791	4.752370
247.859809	7777.339630	14.405939	-0.051817	4.750008
247.920762	7769.310828	14.410944	-0.051823	4.747628
247.720020	7761.364306	14.415949	-0.051781	4.745272
247.793807	7753.336306	14.420954	-0.051790	4.742889
247.694608	7745.330535	14.425959	-0.051766	4.740513
247.902645	7737.397043	14.430963	-0.051800	4.738156
247.657881	7729.303349	14.435968	-0.051749	4.735751
247.620450	7721.367022	14.440973	-0.051738	4.733392
247.415987	7713.286214	14.445978	-0.051695	4.730988
247.346268	7705.315707	14.450983	-0.051677	4.728616
247.194406	7697.348494	14.455987	-0.051643	4.726244
247.037757	7689.274257	14.460992	-0.051609	4.723839
246.999141	7681.362282	14.465997	-0.051597	4.721481
247.106534	7673.291204	14.471002	-0.051612	4.719073
247.165828	7665.347247	14.476007	-0.051618	4.716703
247.187036	7657.326458	14.481011	-0.051617	4.714308
246.886683	7649.291546	14.486016	-0.051556	4.711909
247.197497	7641.283285	14.491021	-0.051609	4.709515
247.247327	7633.288520	14.496026	-0.051613	4.707124
246.885926	7625.285424	14.501031	-0.051541	4.704731
246.930358	7617.350947	14.506035	-0.051544	4.702356
246.958479	7609.316127	14.511040	-0.051545	4.699950
246.885370	7601.371208	14.516045	-0.051526	4.697570
246.708638	7593.271412	14.521050	-0.051488	4.695142
246.804841	7585.246287	14.526055	-0.051501	4.692735
246.614098	7577.272384	14.531059	-0.051461	4.690343
246.639219	7569.234254	14.536064	-0.051460	4.687929
246.500102	7561.278292	14.541069	-0.051430	4.685540
246.672895	7553.302211	14.546074	-0.051457	4.683142
246.440229	7545.269864	14.551079	-0.051408	4.680728
246.526363	7537.292160	14.556083	-0.051420	4.678327
246.402736	7529.319561	14.561088	-0.051392	4.675928
246.693612	7521.258768	14.566093	-0.051441	4.673500
246.542995	7513.130643	14.571098	-0.051408	4.671051
246.455102	7505.195550	14.576103	-0.051386	4.668659
246.357925	7497.210718	14.581107	-0.051363	4.666250
246.181079	7489.158373	14.586112	-0.051325	4.663821
246.151174	7481.257644	14.591117	-0.051315	4.661435
246.291812	7473.224178	14.596122	-0.051336	4.659008
246.155666	7465.287882	14.601127	-0.051306	4.656609
246.159521	7457.225107	14.606131	-0.051301	4.654171
245.943016	7449.163838	14.611136	-0.051256	4.651732
246.277384	7441.214634	14.616141	-0.051313	4.649325
246.055564	7433.234991	14.621146	-0.051267	4.646909
245.968878	7425.179585	14.626151	-0.051246	4.644468
245.826014	7417.283770	14.631155	-0.051215	4.642074
245.844706	7409.195908	14.636160	-0.051213	4.639620
245.919018	7401.257420	14.641165	-0.051222	4.637211
245.861303	7393.210792	14.646170	-0.051206	4.634767
245.833032	7385.179779	14.651175	-0.051196	4.632327
245.701592	7377.193955	14.656179	-0.051167	4.629899
245.604238	7369.184709	14.661184	-0.051143	4.627463
245.734024	7361.183002	14.666189	-0.051163	4.625028
245.684891	7353.206871	14.671194	-0.051148	4.622599
245.603307	7345.168348	14.676199	-0.051128	4.620150
245.703880	7337.212004	14.681203	-0.051142	4.617725
245.627516	7329.156423	14.686208	-0.051123	4.615268
245.557743	7321.216663	14.691213	-0.051105	4.612846
245.391363	7313.108360	14.696218	-0.051069	4.610370
245.556747	7305.160661	14.701223	-0.051095	4.607943
245.308753	7297.166309	14.706227	-0.051044	4.605499
245.208015	7289.143512	14.711232	-0.051020	4.603046
245.380707	7281.173719	14.716237	-0.051047	4.600608
245.229020	7273.178928	14.721242	-0.051014	4.598161
244.907734	7265.159153	14.726247	-0.050949	4.595704
245.202370	7257.139733	14.731251	-0.050999	4.593247
245.095679	7249.088586	14.736256	-0.050974	4.590778
245.275062	7241.130774	14.741261	-0.051003	4.588337
245.125915	7233.106682	14.746266	-0.050970	4.585874
245.020155	7225.126499	14.751271	-0.050945	4.583423
245.072725	7217.157331	14.756275	-0.050950	4.580975
244.960819	7209.144140	14.761280	-0.050924	4.578511
244.904264	7201.200088	14.766285	-0.050909	4.576068
244.831687	7193.140690	14.771290	-0.050890	4.573587
244.928260	7185.092224	14.776295	-0.050903	4.571109
244.860833	7177.147959	14.781299	-0.050886	4.568661
244.782422	7169.093613	14.786304	-0.050866	4.566178
244.718101	7161.152921	14.791309	-0.050849	4.563729
244.621893	7153.168110	14.796314	-0.050826	4.561265
244.728717	7145.125114	14.801319	-0.050841	4.558782
244.873839	7137.195406	14.806323	-0.050863	4.556332
244.580787	7129.095281	14.811328	-0.050804	4.553828
244.797897	7121.069880	14.816333	-0.050839	4.551346
244.565454	7113.056127	14.821338	-0.050791	4.548866
244.295015	7105.097451	14.826343	-0.050736	4.546402
244.615293	7097.094607	14.831347	-0.050790	4.543923
244.689436	7089.144746	14.836352	-0.050799	4.541459
244.579190	7081.128807	14.841357	-0.050774	4.538973
244.338347	7073.120119	14.846362	-0.050724	4.536488
244.401009	7065.096923	14.851367	-0.050730	4.533997
244.567943	7057.125674	14.856371	-0.050757	4.531521
244.412197	7049.070495	14.861376	-0.050723	4.529018
244.375916	7041.142472	14.866381	-0.050711	4.526552
244.372246	7033.126271	14.871386	-0.050705	4.524058
244.116653	7025.147408	14.876391	-0.050653	4.521573
244.251939	7017.131048	14.881395	-0.050673	4.519077
244.033764	7009.172849	14.886400	-0.050627	4.516596
243.895481	7001.128408	14.891405	-0.050597	4.514087
243.821222	6993.002957	14.896410	-0.050578	4.511552
244.016947	6985.001864	14.901415	-0.050609	4.509055
244.034428	6977.065591	14.906419	-0.050608	4.506576
243.818370	6969.018850	14.911424	-0.050562	4.504060
243.881116	6961.113979	14.916429	-0.050569	4.501589
243.917052	6953.047079	14.921434	-0.050571	4.499065
243.855384	6945.074331	14.926439	-0.050554	4.496569
243.636004	6937.078625	14.931443	-0.050508	4.494064
243.580094	6929.040094	14.936448	-0.050493	4.491544
243.541191	6921.037787	14.941453	-0.050481	4.489035
243.272265	6913.066146	14.946458	-0.050426	4.486533
243.511564	6905.033253	14.951463	-0.050465	4.484012
243.540532	6897.108322	14.956467	-0.050466	4.481523
243.507755	6889.047422	14.961472	-0.050455	4.478989
243.424544	6881.091892	14.966477	-0.050434	4.476487
243.441621	6873.046507	14.971482	-0.050433	4.473956
243.134714	6865.020187	14.976487	-0.050370	4.471428
243.177968	6857.033214	14.981491	-0.050373	4.468912
243.187234	6848.988731	14.986496	-0.050370	4.466377
243.327524	6841.017557	14.991501	-0.050391	4.463864
243.223291	6833.057692	14.996506	-0.050367	4.461352
243.231851	6825.042666	15.001511	-0.050364	4.458821
243.326822	6817.062750	15.006515	-0.050376	4.456301
242.980344	6809.009882	15.011520	-0.050307	4.453754
242.860783	6800.975665	15.016525	-0.050280	4.451213
243.036648	6792.997523	15.021530	-0.050307	4.448689
242.884353	6785.004476	15.026535	-0.050274	4.446158
242.854504	6777.035115	15.031539	-0.050264	4.443633
242.804368	6769.031189	15.036544	-0.050249	4.441096
242.861365	6761.069766	15.041549	-0.050255	4.438571
242.625712	6753.082485	15.046554	-0.050206	4.436035
242.730565	6744.966325	15.051559	-0.050221	4.433459
242.886945	6736.956285	15.056563	-0.050245	4.430915
242.758833	6728.940167	15.061568	-0.050216	4.428366
242.598092	6720.972375	15.066573	-0.050181	4.425831
242.629168	6712.991668	15.071578	-0.050182	4.423291
242.778780	6704.999059	15.076583	-0.050205	4.420746
242.517518	6697.000592	15.081587	-0.050151	4.418197
242.458545	6688.961643	15.086592	-0.050135	4.415634
242.562727	6680.969858	15.091597	-0.050150	4.413085
242.314293	6672.958884	15.096602	-0.050098	4.410527
242.372057	6664.973183	15.101607	-0.050104	4.407977
242.422483	6656.958021	15.106611	-0.050109	4.405416
241.987876	6648.964227	15.111616	-0.050023	4.402857
242.001788	6641.037101	15.116621	-0.050020	4.400321
241.935691	6633.034961	15.121626	-0.050003	4.397759
241.902880	6624.968744	15.126631	-0.049992	4.395176
242.044973	6616.998758	15.131635	-0.050013	4.392622
241.881539	6608.916990	15.136640	-0.049978	4.390030
242.025605	6600.997125	15.141645	-0.050000	4.387489
241.950682	6592.964157	15.146650	-0.049981	4.384910
242.006365	6584.988995	15.151655	-0.049986	4.382348
241.989595	6577.017850	15.156659	-0.049978	4.379786
241.953541	6568.979924	15.161664	-0.049967	4.377201
241.997911	6560.981167	15.166669	-0.049970	4.374627
241.831285	6553.010435	15.171674	-0.049934	4.372059
241.742652	6544.949990	15.176679	-0.049912	4.369462
241.763210	6536.972655	15.181683	-0.049911	4.366890
241.547543	6528.963930	15.186688	-0.049866	4.364306
241.689977	6521.053643	15.191693	-0.049888	4.361753
241.747890	6513.010433	15.196698	-0.049893	4.359156
241.632291	6505.034360	15.201703	-0.049867	4.356578
241.702517	6496.990804	15.206707	-0.049875	4.353978
241.503269	6488.887063	15.211712	-0.049833	4.351355
241.288449	6480.890809	15.216717	-0.049788	4.348765
241.290135	6472.923854	15.221722	-0.049783	4.346184
241.517453	6464.960794	15.226727	-0.049821	4.343605
241.348354	6456.985685	15.231731	-0.049784	4.341017
241.224199	6448.961554	15.236736	-0.049756	4.338412
241.328751	6440.961437	15.241741	-0.049771	4.335816
241.208585	6432.972851	15.246746	-0.049743	4.333219
241.033240	6424.925986	15.251751	-0.049706	4.330602
241.154954	6416.984997	15.256755	-0.049723	4.328020
241.084853	6408.958985	15.261760	-0.049705	4.325407
241.011903	6400.960922	15.266765	-0.049687	4.322802
240.987145	6392.974292	15.271770	-0.049677	4.320199
240.778367	6384.958393	15.276775	-0.049633	4.317584
240.672861	6376.950811	15.281779	-0.049609	4.314970
240.605481	6368.948205	15.286784	-0.049591	4.312357
240.675374	6360.917663	15.291789	-0.049599	4.309734
240.441659	6352.930641	15.296794	-0.049551	4.307122
240.505893	6344.930048	15.301799	-0.049558	4.304506
240.636545	6336.972767	15.306803	-0.049577	4.301902
240.591146	6328.917755	15.311808	-0.049564	4.299264
240.417926	6320.982262	15.316813	-0.049527	4.296663
240.410826	6312.898131	15.321818	-0.049520	4.294012
240.354706	6304.889659	15.326823	-0.049505	4.291384
240.449031	6296.907099	15.331827	-0.049517	4.288765
240.332645	6288.909014	15.336832	-0.049491	4.286137
240.398621	6280.919828	15.341837	-0.049498	4.283511
240.224345	6272.941637	15.346842	-0.049461	4.280886
240.143085	6264.945166	15.351847	-0.049441	4.278254
240.001225	6256.957119	15.356851	-0.049409	4.275622
239.880138	6248.894893	15.361856	-0.049382	4.272965
239.871790	6240.867913	15.366861	-0.049375	4.270318
239.783436	6232.892499	15.371866	-0.049354	4.267687
239.842301	6224.853837	15.376871	-0.049360	4.265033
239.820564	6216.962164	15.381875	-0.049351	4.262427
239.694038	6208.919523	15.386880	-0.049322	4.259767
239.740343	6200.921615	15.391885	-0.049326	4.257123
239.602072	6192.926177	15.396890	-0.049295	4.254475
239.683943	6184.893889	15.401895	-0.049305	4.251816
239.842627	6176.891782	15.406899	-0.049330	4.249167
239.557022	6168.894803	15.411904	-0.049272	4.246513
239.637796	6160.906736	15.416909	-0.049282	4.243863
239.625656	6152.930027	15.421914	-0.049275	4.241215
239.769664	6144.959492	15.426919	-0.049297	4.238569
239.752643	6136.955318	15.431923	-0.049288	4.235908
239.453611	6128.909923	15.436928	-0.049228	4.233230
239.636049	6120.910113	15.441933	-0.049257	4.230569
239.629357	6112.948932	15.446938	-0.049250	4.227918
239.295200	6104.916254	15.451943	-0.049183	4.225238
239.283907	6096.997159	15.456947	-0.049176	4.222597
239.190479	6088.929269	15.461952	-0.049154	4.219905
239.395654	6080.960416	15.466957	-0.049187	4.217246
239.242514	6072.954115	15.471962	-0.049154	4.214570
239.346277	6064.902189	15.476967	-0.049168	4.211880
239.339167	6056.940883	15.481971	-0.049162	4.209216
239.154659	6048.929494	15.486976	-0.049122	4.206533
239.093279	6040.956747	15.491981	-0.049106	4.203862
239.083917	6032.980022	15.496986	-0.049099	4.201189
238.892430	6024.934079	15.501991	-0.049059	4.198489
239.032668	6016.985203	15.506995	-0.049080	4.195823
239.100525	6008.840081	15.512000	-0.049087	4.193088
238.984114	6000.834338	15.517005	-0.049061	4.190397
238.796230	5992.866729	15.522010	-0.049021	4.187716
238.888741	5984.863673	15.527015	-0.049033	4.185025
238.852696	5976.958000	15.532019	-0.049021	4.182363
238.568484	5968.884862	15.537024	-0.048963	4.179640
238.694499	5960.927634	15.542029	-0.048982	4.176960
238.854251	5952.919758	15.547034	-0.049007	4.174260
238.490218	5944.904906	15.552039	-0.048934	4.171551
238.526591	5936.915235	15.557043	-0.048936	4.168853
238.631258	5928.882247	15.562048	-0.048950	4.166139
238.678665	5920.898855	15.567053	-0.048954	4.163440
238.463640	5912.946196	15.572058	-0.048909	4.160746
238.346179	5904.903262	15.577063	-0.048882	4.158022
238.485066	5896.928640	15.582067	-0.048903	4.155321
238.329934	5888.907699	15.587072	-0.048869	4.152600
238.360722	5880.874552	15.592077	-0.048870	4.149874
238.182365	5872.879764	15.597082	-0.048832	4.147158
237.929364	5864.886502	15.602087	-0.048780	4.144439
238.007426	5856.917129	15.607091	-0.048789	4.141731
238.217663	5848.849139	15.612096	-0.048824	4.138989
238.176463	5840.904550	15.617101	-0.048811	4.136284
238.122738	5832.870345	15.622106	-0.048796	4.133547
237.866888	5824.837842	15.627111	-0.048743	4.130805
238.106476	5816.886948	15.632115	-0.048783	4.128096
237.949521	5808.885320	15.637120	-0.048749	4.125363
238.011749	5800.933983	15.642125	-0.048755	4.122649
238.024551	5792.904770	15.647130	-0.048753	4.119905
237.805672	5784.930609	15.652135	-0.048707	4.117175
237.566167	5776.898768	15.657139	-0.048658	4.114423
237.573358	5768.855827	15.662144	-0.048654	4.111669
237.902566	5760.831591	15.667149	-0.048710	4.108923
237.751838	5752.847230	15.672154	-0.048677	4.106183
237.515853	5744.865161	15.677159	-0.048628	4.103441
237.569359	5736.935576	15.682163	-0.048633	4.100719
237.494443	5728.945354	15.687168	-0.048614	4.097973
237.394286	5720.928828	15.692173	-0.048591	4.095215
237.325004	5712.878449	15.697178	-0.048573	4.092444
237.294175	5704.867402	15.702183	-0.048562	4.089686
237.165676	5696.931755	15.707187	-0.048533	4.086950
237.202283	5688.912569	15.712192	-0.048535	4.084186
237.239704	5680.960285	15.717197	-0.048537	4.081443
237.314813	5672.973863	15.722202	-0.048546	4.078687
237.261499	5664.957320	15.727207	-0.048531	4.075917
237.494597	5656.922057	15.732211	-0.048570	4.073142
237.219683	5648.894739	15.737216	-0.048514	4.070361
237.055748	5640.948744	15.742221	-0.048478	4.067608
236.964502	5632.938557	15.747226	-0.048456	4.064832
237.065722	5624.961982	15.752231	-0.048470	4.062069
236.966567	5616.936102	15.757235	-0.048447	4.059283
236.892868	5608.965071	15.762240	-0.048428	4.056515
236.969340	5600.963604	15.767245	-0.048437	4.053737
237.030898	5592.911658	15.772250	-0.048444	4.050939
236.835790	5584.927205	15.777255	-0.048402	4.048159
236.669961	5576.953362	15.782259	-0.048366	4.045381
236.643118	5568.993503	15.787264	-0.048357	4.042608
236.595389	5560.953163	15.792269	-0.048343	4.039805
236.434646	5552.985910	15.797274	-0.048308	4.037023
236.482955	5544.916862	15.802279	-0.048312	4.034208
236.414892	5536.832558	15.807283	-0.048294	4.031383
236.574965	5528.837792	15.812288	-0.048319	4.028591
236.562304	5520.882817	15.817293	-0.048312	4.025808
236.555688	5512.922389	15.822298	-0.048305	4.023022
236.520892	5504.892099	15.827303	-0.048294	4.020209
236.524980	5496.927169	15.832307	-0.048290	4.017417
236.271802	5488.932052	15.837312	-0.048238	4.014609
235.960269	5480.932797	15.842317	-0.048175	4.011796
236.136351	5472.929876	15.847322	-0.048203	4.008988
236.082372	5464.901119	15.852327	-0.048187	4.006165
236.209509	5456.930198	15.857331	-0.048206	4.003363
235.957058	5448.914657	15.862336	-0.048154	4.000538
236.052771	5440.939522	15.867341	-0.048167	3.997730
236.046253	5432.943647	15.872346	-0.048161	3.994912
236.040248	5424.913587	15.877351	-0.048155	3.992079
235.913673	5416.907179	15.882355	-0.048126	3.989251
235.749227	5408.912683	15.887360	-0.048091	3.986424
235.799956	5400.915681	15.892365	-0.048095	3.983598
235.693627	5392.948444	15.897370	-0.048070	3.980778
235.681882	5384.933975	15.902375	-0.048063	3.977941
235.634911	5376.961255	15.907379	-0.048050	3.975116
235.632138	5368.905861	15.912384	-0.048044	3.972260
235.756742	5360.895081	15.917389	-0.048062	3.969420
235.632626	5352.942294	15.922394	-0.048034	3.966595
235.482626	5344.929709	15.927399	-0.048001	3.963746
235.688905	5337.012034	15.932403	-0.048035	3.960934
235.687053	5328.970476	15.937408	-0.048029	3.958073
235.339270	5321.043554	15.942413	-0.047960	3.955245
235.362209	5312.962505	15.947418	-0.047959	3.952366
235.456468	5304.886481	15.952423	-0.047972	3.949488
235.404164	5296.985314	15.957427	-0.047957	3.946668
235.099330	5288.980772	15.962432	-0.047895	3.943805
235.146369	5281.004953	15.967437	-0.047899	3.940956
235.339276	5273.000590	15.972442	-0.047930	3.938097
235.215221	5264.985495	15.977447	-0.047902	3.935226
235.212731	5256.984167	15.982451	-0.047896	3.932361
235.126693	5248.923208	15.987456	-0.047875	3.929471
235.060432	5241.012550	15.992461	-0.047858	3.926632
234.901313	5233.045389	15.997466	-0.047824	3.923770
235.077615	5225.009722	16.002471	-0.047851	3.920887
235.150988	5217.032903	16.007475	-0.047860	3.918022
234.836710	5209.001918	16.012480	-0.047797	3.915127
234.817585	5200.977449	16.017485	-0.047788	3.912238
235.067599	5192.959766	16.022490	-0.047830	3.909355
234.572939	5185.028013	16.027495	-0.047733	3.906486
234.708664	5176.998602	16.032499	-0.047753	3.903592
234.687554	5168.965123	16.037504	-0.047744	3.900692
234.618411	5161.024801	16.042509	-0.047726	3.897822
234.452962	5153.024646	16.047514	-0.047690	3.894926
234.508451	5144.962800	16.052519	-0.047696	3.892010
234.639443	5136.960726	16.057523	-0.047715	3.889115
234.476759	5129.001696	16.062528	-0.047680	3.886228
234.563512	5121.004373	16.067533	-0.047691	3.883329
234.589429	5113.015386	16.072538	-0.047691	3.880431
234.353452	5105.038699	16.077543	-0.047642	3.877529
234.230358	5097.018212	16.082547	-0.047614	3.874611
234.075969	5088.732682	16.087552	-0.047580	3.871595
234.067248	5080.827278	16.092557	-0.047574	3.868717
234.217682	5072.899390	16.097562	-0.047597	3.865832
234.288861	5064.935469	16.102567	-0.047605	3.862930
234.259759	5056.954784	16.107571	-0.047595	3.860018
234.033561	5049.013217	16.112576	-0.047548	3.857114
234.269826	5041.023993	16.117581	-0.047587	3.854199
234.102377	5033.004215	16.122586	-0.047551	3.851263
234.010493	5024.959136	16.127591	-0.047528	3.848317
233.821904	5017.021105	16.132595	-0.047488	3.845406
233.895217	5009.001265	16.137600	-0.047497	3.842469
234.103797	5001.025024	16.142605	-0.047531	3.839547
233.840311	4993.093306	16.147610	-0.047477	3.836630
233.739191	4985.060000	16.152615	-0.047453	3.833677
233.862985	4977.026098	16.157619	-0.047471	3.830726
233.696080	4969.008125	16.162624	-0.047435	3.827773
233.749576	4961.043990	16.167629	-0.047440	3.824842
233.767797	4953.053244	16.172634	-0.047439	3.821898
233.515055	4945.068176	16.177639	-0.047387	3.818948
233.381723	4937.113782	16.182643	-0.047357	3.816009
233.357218	4929.077309	16.187648	-0.047347	3.813041
233.394713	4921.066301	16.192653	-0.047349	3.810080
233.402631	4913.085169	16.197658	-0.047346	3.807128
233.318123	4905.081080	16.202663	-0.047325	3.804163
233.359371	4897.143273	16.207667	-0.047328	3.801223
233.282897	4889.126790	16.212672	-0.047309	3.798249
233.271124	4881.112799	16.217677	-0.047301	3.795275
233.359914	4873.087371	16.222682	-0.047313	3.792297
232.961113	4865.035939	16.227687	-0.047234	3.789295
232.888930	4857.103287	16.232691	-0.047215	3.786343
232.909335	4849.079931	16.237696	-0.047214	3.783357
232.923091	4841.107704	16.242701	-0.047212	3.780387
232.854288	4833.129979	16.247706	-0.047194	3.777412
232.821116	4825.084493	16.252711	-0.047183	3.774409
233.046321	4817.066522	16.257715	-0.047220	3.771420
232.972253	4809.081384	16.262720	-0.047201	3.768434
232.711083	4801.139070	16.267725	-0.047147	3.765457
232.688818	4793.128492	16.272730	-0.047138	3.762458
232.555441	4785.119482	16.277735	-0.047108	3.759455
232.668545	4777.190807	16.282739	-0.047125	3.756485
232.506596	4769.119024	16.287744	-0.047089	3.753453
232.515186	4761.110576	16.292749	-0.047086	3.750446
232.511714	4753.090205	16.297754	-0.047080	3.747431
232.290563	4745.099009	16.302759	-0.047034	3.744420
232.519727	4737.125112	16.307763	-0.047072	3.741424
232.254932	4729.125575	16.312768	-0.047018	3.738404
232.139222	4721.166272	16.317773	-0.046991	3.735401
232.413694	4713.129224	16.322778	-0.047037	3.732375
232.370963	4705.083153	16.327783	-0.047024	3.729335
232.188871	4697.167298	16.332787	-0.046986	3.726339
232.105981	4689.157515	16.337792	-0.046965	3.723307
232.049509	4681.182285	16.342797	-0.046950	3.720286
231.911815	4673.254191	16.347802	-0.046919	3.717279
231.784009	4665.187918	16.352807	-0.046890	3.714218
232.166944	4657.090457	16.357811	-0.046957	3.711154
231.866994	4649.127537	16.362816	-0.046896	3.708122
231.868323	4641.150062	16.367821	-0.046891	3.705090
231.697841	4633.196055	16.372826	-0.046854	3.702060
231.881389	4625.155847	16.377831	-0.046884	3.699003
231.655289	4617.261243	16.382835	-0.046837	3.695989
231.586017	4609.215590	16.387840	-0.046819	3.692919
231.802717	4601.179894	16.392845	-0.046854	3.689857
231.623018	4593.231709	16.397850	-0.046816	3.686816
231.362933	4585.204078	16.402855	-0.046762	3.683740
231.520383	4577.255010	16.407859	-0.046787	3.680703
231.311640	4569.274111	16.412864	-0.046743	3.677641
231.271585	4561.234126	16.417869	-0.046730	3.674558
231.551159	4553.229101	16.422874	-0.046777	3.671495
231.399798	4545.201097	16.427879	-0.046744	3.668408
231.252687	4537.246231	16.432883	-0.046712	3.665348
231.130215	4529.242856	16.437888	-0.046684	3.662267
231.125298	4521.261004	16.442893	-0.046678	3.659194
231.104800	4513.307175	16.447898	-0.046670	3.656130
230.864085	4505.261737	16.452903	-0.046620	3.653022
231.058085	4497.267110	16.457907	-0.046651	3.649942
231.227188	4489.229954	16.462912	-0.046677	3.646842
231.025249	4481.243657	16.467917	-0.046635	3.643750
230.941783	4473.308493	16.472922	-0.046614	3.640678
230.771959	4465.308672	16.477927	-0.046578	3.637576
230.882232	4457.297932	16.482931	-0.046593	3.634474
230.648558	4449.254355	16.487936	-0.046545	3.631348
230.578724	4441.257028	16.492941	-0.046527	3.628242
230.658644	4433.265748	16.497946	-0.046537	3.625139
230.603709	4425.293147	16.502951	-0.046522	3.622038
230.576720	4417.315016	16.507955	-0.046512	3.618932
230.412520	4409.339810	16.512960	-0.046476	3.615821
230.455457	4401.316073	16.517965	-0.046479	3.612694
230.463617	4393.303335	16.522970	-0.046476	3.609567
230.445186	4385.320208	16.527975	-0.046467	3.606449
230.578080	4377.336400	16.532979	-0.046487	3.603332
230.266313	4369.351359	16.537984	-0.046424	3.600200
230.247323	4361.408209	16.542989	-0.046416	3.597089
230.339631	4353.373167	16.547994	-0.046428	3.593942
230.278228	4345.332338	16.552999	-0.046411	3.590787
230.131874	4337.385828	16.558003	-0.046379	3.587663
230.296128	4329.364236	16.563008	-0.046405	3.584516
230.174638	4321.417199	16.568013	-0.046377	3.581387
230.081744	4313.406112	16.573018	-0.046355	3.578231
229.819308	4305.406604	16.578023	-0.046301	3.575071
229.830525	4297.425902	16.583027	-0.046298	3.571925
229.533306	4289.401352	16.588032	-0.046238	3.568749
229.601426	4281.413269	16.593037	-0.046246	3.565596
229.740514	4273.448298	16.598042	-0.046267	3.562450
229.570001	4265.443039	16.603047	-0.046230	3.559278
229.466679	4257.514860	16.608051	-0.046206	3.556134
229.606204	4249.380456	16.613056	-0.046227	3.552914
229.356390	4241.352410	16.618061	-0.046175	3.549721
229.497372	4233.392834	16.623066	-0.046196	3.546564
229.348498	4225.395295	16.628071	-0.046164	3.543380
229.357391	4217.442567	16.633075	-0.046160	3.540216
229.188531	4209.466464	16.638080	-0.046124	3.537035
229.263264	4201.437716	16.643085	-0.046133	3.533837
229.313972	4193.424284	16.648090	-0.046137	3.530642
229.209857	4185.415781	16.653095	-0.046113	3.527441
229.249565	4177.438784	16.658099	-0.046115	3.524254
229.063961	4169.523633	16.663104	-0.046076	3.521082
229.017534	4161.492823	16.668109	-0.046062	3.517865
228.902337	4153.514372	16.673114	-0.046036	3.514664
228.785400	4145.486591	16.678119	-0.046009	3.511440
229.110359	4137.493565	16.683123	-0.046065	3.508241
228.914964	4129.464050	16.688128	-0.046023	3.505008
228.837257	4121.522909	16.693133	-0.046004	3.501812
228.970407	4113.533147	16.698138	-0.046024	3.498599
228.770541	4105.553374	16.703143	-0.045982	3.495377
228.930737	4097.568414	16.708147	-0.046006	3.492162
228.855457	4089.532651	16.713152	-0.045987	3.488915
228.883817	4081.571951	16.718157	-0.045988	3.485699
228.788605	4073.602080	16.723162	-0.045965	3.482473
228.729429	4065.605969	16.728167	-0.045949	3.479233
228.799602	4057.652547	16.733171	-0.045957	3.476013
228.435241	4049.611648	16.738176	-0.045884	3.472740
228.247344	4041.602918	16.743181	-0.045844	3.469482
228.398686	4033.587842	16.748186	-0.045868	3.466230
228.251523	4025.587940	16.753191	-0.045835	3.462971
228.253020	4017.637397	16.758195	-0.045831	3.459734
228.193588	4009.654772	16.763200	-0.045815	3.456479
228.190577	4001.622377	16.768205	-0.045809	3.453203
228.307489	3993.608582	16.773210	-0.045826	3.449935
228.120612	3985.623056	16.778215	-0.045786	3.446665
228.179845	3977.666461	16.783219	-0.045792	3.443412
228.112143	3969.688797	16.788224	-0.045775	3.440143
228.007749	3961.677577	16.793229	-0.045750	3.436857
227.927760	3953.707073	16.798234	-0.045730	3.433584
227.846249	3945.647825	16.803239	-0.045710	3.430272
227.986207	3937.673910	16.808243	-0.045731	3.426999
228.008082	3929.649749	16.813248	-0.045730	3.423699
227.841486	3921.723094	16.818253	-0.045694	3.420429
227.840724	3913.751809	16.823258	-0.045689	3.417143
227.887839	3905.724490	16.828263	-0.045693	3.413832
227.772664	3897.747105	16.833267	-0.045667	3.410533
227.582359	3889.745246	16.838272	-0.045626	3.407219
227.565025	3881.770791	16.843277	-0.045618	3.403918
227.537244	3873.801942	16.848282	-0.045608	3.400616
227.338618	3865.819775	16.853287	-0.045566	3.397300
227.359165	3857.808319	16.858291	-0.045565	3.393976
227.414833	3849.695097	16.863296	-0.045570	3.390607
227.404574	3841.735039	16.868301	-0.045563	3.387296
227.319431	3833.777852	16.873306	-0.045543	3.383981
227.346883	3825.799504	16.878311	-0.045543	3.380658
227.564158	3817.809146	16.883315	-0.045578	3.377333
227.432240	3809.817388	16.888320	-0.045549	3.373992
227.434082	3801.805784	16.893325	-0.045544	3.370644
227.209889	3793.867700	16.898330	-0.045497	3.367315
227.193768	3785.831083	16.903335	-0.045489	3.363949
226.992166	3777.912981	16.908339	-0.045447	3.360623
226.878471	3769.924605	16.913344	-0.045421	3.357267
226.924678	3761.902259	16.918349	-0.045424	3.353899
226.748058	3753.875287	16.923354	-0.045387	3.350518
226.672829	3745.884800	16.928359	-0.045368	3.347153
226.673554	3737.900242	16.933363	-0.045363	3.343789
226.481079	3729.927205	16.938368	-0.045322	3.340420
226.608343	3721.935177	16.943373	-0.045341	3.337051
226.634434	3713.903878	16.948378	-0.045341	3.333658
226.562868	3705.884870	16.953383	-0.045322	3.330264
226.513430	3697.958358	16.958387	-0.045308	3.326906
226.447059	3689.967008	16.963392	-0.045291	3.323516
226.598703	3681.977870	16.968397	-0.045314	3.320132
226.602424	3673.990771	16.973402	-0.045310	3.316740
226.243261	3665.999195	16.978407	-0.045238	3.313329
226.318208	3657.976782	16.983411	-0.045247	3.309918
226.377888	3649.982275	16.988416	-0.045253	3.306514
226.343099	3642.002196	16.993421	-0.045242	3.303109
226.370843	3634.015280	16.998426	-0.045242	3.299701
226.131287	3626.072938	17.003431	-0.045192	3.296298
226.183639	3618.076269	17.008435	-0.045197	3.292879
225.948164	3610.053273	17.013440	-0.045148	3.289434
226.019589	3602.071572	17.018445	-0.045157	3.286015
225.794295	3594.126381	17.023450	-0.045110	3.282597
225.606825	3586.122964	17.028455	-0.045070	3.279151
225.886065	3578.130735	17.033459	-0.045117	3.275725
225.817947	3570.107256	17.038464	-0.045099	3.272268
225.835714	3562.104023	17.043469	-0.045098	3.268820
225.809075	3554.145829	17.048474	-0.045088	3.265386
225.901074	3546.131710	17.053479	-0.045100	3.261929
225.731483	3538.177436	17.058483	-0.045063	3.258483
225.445981	3530.188227	17.063488	-0.045005	3.255014
225.671860	3522.149828	17.068493	-0.045042	3.251541
225.699786	3514.178452	17.073498	-0.045042	3.248085
225.401396	3506.188917	17.078503	-0.044982	3.244604
225.477207	3498.248844	17.083507	-0.044991	3.241156
225.625904	3490.240862	17.088512	-0.045014	3.237678
225.415585	3482.246134	17.093517	-0.044970	3.234187
225.156117	3474.236813	17.098522	-0.044916	3.230684
224.902992	3466.226424	17.103527	-0.044864	3.227177
225.146582	3458.232674	17.108531	-0.044905	3.223694
225.017636	3450.245276	17.113536	-0.044876	3.220195
225.005597	3442.284858	17.118541	-0.044869	3.216708
224.915710	3434.305533	17.123546	-0.044847	3.213206
224.891147	3426.270496	17.128551	-0.044837	3.209678
224.819820	3418.310509	17.133555	-0.044819	3.206178
224.555553	3410.354825	17.138560	-0.044765	3.202668
224.639414	3402.352994	17.143565	-0.044776	3.199148
224.892213	3394.377845	17.148570	-0.044818	3.195643
224.867313	3386.349402	17.153575	-0.044808	3.192098
224.776640	3378.370070	17.158579	-0.044786	3.188569
224.279238	3370.398318	17.163584	-0.044689	3.185022
224.441953	3362.419629	17.168589	-0.044714	3.181496
224.627934	3354.425654	17.173594	-0.044744	3.177961
224.546069	3346.414936	17.178599	-0.044723	3.174402
224.383799	3338.449793	17.183603	-0.044688	3.170857
224.414184	3330.434338	17.188608	-0.044689	3.167293
224.350999	3322.460776	17.193613	-0.044672	3.163740
224.226297	3314.525972	17.198618	-0.044644	3.160197
224.268023	3306.511238	17.203623	-0.044647	3.156622
224.252712	3298.520200	17.208627	-0.044639	3.153051
224.136815	3290.479680	17.213632	-0.044613	3.149450
224.283416	3282.501483	17.218637	-0.044635	3.145883
224.219670	3274.531297	17.223642	-0.044618	3.142308
224.022727	3266.547144	17.228647	-0.044576	3.138715
224.039175	3258.554020	17.233651	-0.044574	3.135124
223.961606	3250.566135	17.238656	-0.044555	3.131528
224.046233	3242.554824	17.243661	-0.044566	3.127923
223.852422	3234.619010	17.248666	-0.044525	3.124336
223.768724	3226.653151	17.253671	-0.044504	3.120737
223.721676	3218.687365	17.258675	-0.044491	3.117135
223.469415	3210.677450	17.263680	-0.044439	3.113499
223.466970	3202.655552	17.268685	-0.044433	3.109865
223.545229	3194.674873	17.273690	-0.044443	3.106249
223.312440	3186.692670	17.278695	-0.044395	3.102614
223.337259	3178.725675	17.283699	-0.044394	3.098993
223.432378	3170.718412	17.288704	-0.044407	3.095354
223.423444	3162.724150	17.293709	-0.044400	3.091710
223.480472	3154.731295	17.298714	-0.044406	3.088067
223.278256	3146.719398	17.303719	-0.044363	3.084398
223.519355	3138.778688	17.308723	-0.044403	3.080778
223.067399	3130.831634	17.313728	-0.044314	3.077119
222.908671	3122.827701	17.318733	-0.044280	3.073443
223.089200	3114.729529	17.323738	-0.044308	3.069735
223.087584	3106.762853	17.328743	-0.044303	3.066074
222.937243	3098.847348	17.333747	-0.044270	3.062426
223.011472	3090.850610	17.338752	-0.044279	3.058746
222.648804	3082.902201	17.343757	-0.044207	3.055064
222.574776	3074.912937	17.348762	-0.044188	3.051372
222.579725	3066.889474	17.353767	-0.044184	3.047663
222.686413	3058.915165	17.358771	-0.044199	3.043978
222.606145	3050.934776	17.363776	-0.044179	3.040276
222.447238	3042.989106	17.368781	-0.044144	3.036582
222.668674	3034.955283	17.373786	-0.044180	3.032861
222.488562	3026.945448	17.378791	-0.044142	3.029127
222.508874	3018.993721	17.383795	-0.044141	3.025425
222.329320	3011.026398	17.388800	-0.044102	3.021702
222.445133	3003.027415	17.393805	-0.044119	3.017973
222.523870	2995.037469	17.398810	-0.044129	3.014243
222.244650	2987.057598	17.403815	-0.044072	3.010495
222.298608	2979.066103	17.408819	-0.044077	3.006753
222.232994	2971.090472	17.413824	-0.044060	3.003008
221.981103	2963.131857	17.418829	-0.044008	2.999258
222.155140	2955.182093	17.423834	-0.044035	2.995528
222.121737	2947.142858	17.428839	-0.044024	2.991740
222.175164	2939.153578	17.433843	-0.044029	2.987976
221.997430	2931.145375	17.438848	-0.043991	2.984187
221.979345	2923.183242	17.443853	-0.043983	2.980422
222.092518	2915.234978	17.448858	-0.043999	2.976666
221.778689	2907.255410	17.453863	-0.043935	2.972869
221.862059	2899.251572	17.458867	-0.043946	2.969075
221.662324	2891.271864	17.463872	-0.043904	2.965274
221.399042	2883.319160	17.468877	-0.043850	2.961477
221.492847	2875.342943	17.473882	-0.043862	2.957683
221.576120	2867.306746	17.478887	-0.043873	2.953854
221.528887	2859.319194	17.483891	-0.043859	2.950037
221.239423	2851.369522	17.488896	-0.043800	2.946221
221.539503	2843.336420	17.493901	-0.043851	2.942390
221.470447	2835.386247	17.498906	-0.043833	2.938575
221.201657	2827.427869	17.503911	-0.043778	2.934741
221.347075	2819.413473	17.508915	-0.043800	2.930896
221.443870	2811.406400	17.513920	-0.043814	2.927047
221.183849	2803.472783	17.518925	-0.043760	2.923210
221.239435	2795.495101	17.523930	-0.043766	2.919363
221.206385	2787.527303	17.528935	-0.043754	2.915511
221.113024	2779.470294	17.533939	-0.043732	2.911607
220.966534	2771.480217	17.538944	-0.043700	2.907728
220.903274	2763.498127	17.543949	-0.043683	2.903852
220.961254	2755.562778	17.548954	-0.043689	2.900000
220.906534	2747.573457	17.553959	-0.043674	2.896111
220.969837	2739.584370	17.558963	-0.043681	2.892223
220.751844	2731.611660	17.563968	-0.043635	2.888322
220.620279	2723.631275	17.568973	-0.043606	2.884417
220.644763	2715.707520	17.573978	-0.043605	2.880543
220.762137	2707.689120	17.578983	-0.043622	2.876623
220.637058	2699.719528	17.583987	-0.043594	2.872707
220.515242	2691.716033	17.588992	-0.043566	2.868770
220.464162	2683.727068	17.593997	-0.043552	2.864839
220.352973	2675.808440	17.599002	-0.043526	2.860933
220.152282	2667.802581	17.604007	-0.043484	2.856974
220.143961	2659.827917	17.609011	-0.043477	2.853036
220.277688	2651.800264	17.614016	-0.043497	2.849073
220.088312	2643.854940	17.619021	-0.043457	2.845128
219.985819	2635.907108	17.624026	-0.043433	2.841182
220.109797	2627.895640	17.629031	-0.043451	2.837210
220.131185	2619.913269	17.634035	-0.043450	2.833242
220.062372	2611.900977	17.639040	-0.043432	2.829249
220.071949	2603.932375	17.644045	-0.043429	2.825276
220.046247	2595.983383	17.649050	-0.043419	2.821305
219.861984	2587.999506	17.654055	-0.043380	2.817302
219.923648	2580.021900	17.659059	-0.043387	2.813310
219.928644	2572.022282	17.664064	-0.043383	2.809299
219.575163	2564.076609	17.669069	-0.043312	2.805288
219.585369	2556.115429	17.674074	-0.043309	2.801285
219.597734	2548.121396	17.679079	-0.043306	2.797259
219.518565	2540.163680	17.684083	-0.043287	2.793241
219.456632	2532.154315	17.689088	-0.043270	2.789192
219.494588	2524.169067	17.694093	-0.043272	2.785154
219.680919	2516.202134	17.699098	-0.043302	2.781130
219.448292	2508.241324	17.704103	-0.043254	2.777077
219.399411	2500.267749	17.709107	-0.043240	2.773023
219.489694	2492.242382	17.714112	-0.043251	2.768945
219.308499	2484.280161	17.719117	-0.043213	2.764877
219.114359	2476.371012	17.724122	-0.043172	2.760830
219.167417	2468.382266	17.729127	-0.043177	2.756750
219.013759	2460.366856	17.734131	-0.043143	2.752638
219.133645	2452.327008	17.739136	-0.043160	2.748525
219.038451	2444.351862	17.744141	-0.043138	2.744425
218.859443	2436.445925	17.749146	-0.043099	2.740349
218.770348	2428.464858	17.754151	-0.043078	2.736235
218.863602	2420.481472	17.759155	-0.043090	2.732124
218.824924	2412.497332	17.764160	-0.043078	2.727998
218.653659	2404.542276	17.769165	-0.043041	2.723873
218.564174	2396.590218	17.774170	-0.043020	2.719748
218.482467	2388.639121	17.779175	-0.043000	2.715618
218.575083	2380.621079	17.784179	-0.043012	2.711457
218.493942	2372.635502	17.789184	-0.042992	2.707297
218.305797	2364.682862	17.794189	-0.042952	2.703140
218.429344	2356.704507	17.799194	-0.042970	2.698983
218.222457	2348.739952	17.804199	-0.042926	2.694806
218.000546	2340.786098	17.809203	-0.042880	2.690627
218.327328	2332.736239	17.814208	-0.042936	2.686426
218.196723	2324.811111	17.819213	-0.042907	2.682255
217.992708	2316.894228	17.824218	-0.042864	2.678078
218.125433	2308.868441	17.829223	-0.042883	2.673857
218.277447	2300.818616	17.834227	-0.042907	2.669619
217.969359	2292.882926	17.839232	-0.042844	2.665404
217.846638	2284.943256	17.844237	-0.042817	2.661193
217.779557	2276.990015	17.849242	-0.042799	2.656972
217.715644	2268.985040	17.854247	-0.042782	2.652716
217.807845	2261.010473	17.859251	-0.042795	2.648480
217.695961	2253.028562	17.864256	-0.042769	2.644220
217.835830	2245.072776	17.869261	-0.042790	2.639983
217.768125	2237.133041	17.874266	-0.042772	2.635735
217.661184	2229.123584	17.879271	-0.042748	2.631440
217.791668	2221.147106	17.884275	-0.042767	2.627171
217.399474	2213.213870	17.889280	-0.042689	2.622883
217.407098	2205.242003	17.894285	-0.042685	2.618595
217.425834	2197.276309	17.899290	-0.042684	2.614303
217.404110	2189.253581	17.904295	-0.042675	2.609971
217.171637	2181.338476	17.909299	-0.042627	2.605676
217.140277	2173.366859	17.914304	-0.042616	2.601357
217.128469	2165.400306	17.919309	-0.042609	2.597034
216.929182	2157.359948	17.924314	-0.042567	2.592651
216.843221	2149.269258	17.929319	-0.042546	2.588241
216.991708	2141.328914	17.934323	-0.042568	2.583922
217.078177	2133.382698	17.939328	-0.042579	2.579588
216.946170	2125.461289	17.944333	-0.042550	2.575246
216.887585	2117.505931	17.949338	-0.042534	2.570882
216.839938	2109.531761	17.954343	-0.042520	2.566501
216.744488	2101.600242	17.959347	-0.042498	2.562133
216.687026	2093.660788	17.964352	-0.042482	2.557756
216.800192	2085.661888	17.969357	-0.042498	2.553350
216.745781	2077.689239	17.974362	-0.042483	2.548940
216.527545	2069.718282	17.979367	-0.042437	2.544511
216.663465	2061.775577	17.984371	-0.042458	2.540115
216.511986	2053.826190	17.989376	-0.042425	2.535688
216.360570	2045.858821	17.994381	-0.042392	2.531243
216.347433	2037.882817	17.999386	-0.042384	2.526795
216.241845	2029.920693	18.004391	-0.042360	2.522340
216.292628	2021.983297	18.009395	-0.042364	2.517902
216.102776	2014.009242	18.014400	-0.042324	2.513419
216.324154	2005.961908	18.019405	-0.042360	2.508916
216.377062	1998.001039	18.024410	-0.042365	2.504442
216.226424	1990.073425	18.029415	-0.042332	2.499963
216.161053	1982.133062	18.034419	-0.042315	2.495476
216.159165	1974.146684	18.039424	-0.042309	2.490958
216.037557	1966.173513	18.044429	-0.042282	2.486432
215.952503	1958.250572	18.049434	-0.042261	2.481928
215.799132	1950.295266	18.054439	-0.042228	2.477393
215.760458	1942.339958	18.059443	-0.042215	2.472858
215.735996	1934.328554	18.064448	-0.042206	2.468283
215.562741	1926.387981	18.069453	-0.042169	2.463730
215.513912	1918.437208	18.074458	-0.042155	2.459171
215.605617	1910.447203	18.079463	-0.042167	2.454592
215.774237	1902.465752	18.084467	-0.042193	2.450015
215.420490	1894.543614	18.089472	-0.042122	2.445424
215.492071	1886.577112	18.094477	-0.042131	2.440832
215.369713	1878.661075	18.099482	-0.042103	2.436245
215.581002	1870.584380	18.104487	-0.042138	2.431581
215.440627	1862.621342	18.109491	-0.042106	2.426948
215.161128	1854.698699	18.114496	-0.042049	2.422319
215.183456	1846.739606	18.119501	-0.042049	2.417683
215.151095	1838.784316	18.124506	-0.042038	2.413035
215.116755	1830.803303	18.129511	-0.042026	2.408364
215.209592	1822.856784	18.134515	-0.042039	2.403714
215.062085	1814.932639	18.139520	-0.042006	2.399049
214.723162	1807.026744	18.144525	-0.041938	2.394371
214.724210	1799.017274	18.149530	-0.041934	2.389649
214.811213	1791.015816	18.154535	-0.041945	2.384929
214.827391	1783.092581	18.159539	-0.041943	2.380241
214.474125	1775.175096	18.164544	-0.041872	2.375517
214.522360	1767.187071	18.169549	-0.041876	2.370774
214.471556	1759.239321	18.174554	-0.041862	2.366038
214.289782	1751.292752	18.179559	-0.041823	2.361282
214.399232	1743.337595	18.184563	-0.041838	2.356535
214.681395	1735.311261	18.189568	-0.041886	2.351750
214.416756	1727.372231	18.194573	-0.041832	2.346963
214.481479	1719.426429	18.199578	-0.041839	2.342189
214.379568	1711.476706	18.204583	-0.041815	2.337389
214.365504	1703.540978	18.209587	-0.041807	2.332595
214.258246	1695.562106	18.214592	-0.041783	2.327757
214.010348	1687.645280	18.219597	-0.041731	2.322936
214.078415	1679.694724	18.224602	-0.041739	2.318110
213.757439	1671.766232	18.229607	-0.041674	2.313254
213.874027	1663.777817	18.234611	-0.041691	2.308389
213.674839	1655.836444	18.239616	-0.041649	2.303515
213.713096	1647.869730	18.244621	-0.041651	2.298636
213.947202	1639.898552	18.249626	-0.041690	2.293760
213.654990	1631.955307	18.254631	-0.041631	2.288846
213.730451	1623.995549	18.259635	-0.041640	2.283943
213.665651	1616.071933	18.264640	-0.041623	2.279040
213.605344	1608.121989	18.269645	-0.041607	2.274110
213.628497	1600.084575	18.274650	-0.041606	2.269122
213.357122	1592.161022	18.279655	-0.041551	2.264169
213.225928	1584.247022	18.284659	-0.041521	2.259222
213.336023	1576.279706	18.289664	-0.041537	2.254253
213.321798	1568.307841	18.294669	-0.041529	2.249259
213.124578	1560.395333	18.299674	-0.041487	2.244275
213.035137	1552.460941	18.304679	-0.041466	2.239275
213.024879	1544.530526	18.309683	-0.041459	2.234274
212.842857	1536.557520	18.314688	-0.041420	2.229220
212.601428	1528.618668	18.319693	-0.041370	2.224170
212.795970	1520.663818	18.324698	-0.041402	2.219138
212.560798	1512.726245	18.329703	-0.041353	2.214066
212.663737	1504.760150	18.334707	-0.041367	2.208995
212.409086	1496.841437	18.339712	-0.041315	2.203911
212.434442	1488.885823	18.344717	-0.041315	2.198816
212.508418	1480.946112	18.349722	-0.041323	2.193724
212.404909	1472.959046	18.354727	-0.041299	2.188574
212.417790	1465.027026	18.359731	-0.041297	2.183458
212.135604	1457.131092	18.364736	-0.041239	2.178325
212.183334	1449.160169	18.369741	-0.041243	2.173163
212.329934	1441.197185	18.374746	-0.041265	2.168002
212.175056	1433.261044	18.379751	-0.041232	2.162819
212.088474	1425.370336	18.384755	-0.041211	2.157659
211.906597	1417.423302	18.389760	-0.041172	2.152441
211.738766	1409.475107	18.394765	-0.041136	2.147211
211.885561	1401.531418	18.399770	-0.041158	2.142001
211.701871	1393.608220	18.404775	-0.041119	2.136760
211.784419	1385.644632	18.409779	-0.041129	2.131505
211.622350	1377.712017	18.414784	-0.041094	2.126234
211.630229	1369.779391	18.419789	-0.041091	2.120966
211.564670	1361.870481	18.424794	-0.041074	2.115694
211.520878	1353.857883	18.429799	-0.041061	2.110342
211.267560	1345.947641	18.434803	-0.041009	2.105024
211.302609	1337.999305	18.439808	-0.041010	2.099695
211.351575	1330.071863	18.444813	-0.041014	2.094368
211.489775	1322.113893	18.449818	-0.041035	2.089015
211.292086	1314.193425	18.454823	-0.040993	2.083642
211.253213	1306.287191	18.459827	-0.040981	2.078279
211.037031	1298.380870	18.464832	-0.040936	2.072885
210.861272	1290.437432	18.469837	-0.040898	2.067455
210.808158	1282.513252	18.474842	-0.040884	2.062037
210.564438	1274.607763	18.479847	-0.040833	2.056598
210.727484	1266.646957	18.484851	-0.040859	2.051148
210.698418	1258.700931	18.489856	-0.040848	2.045673
210.747791	1250.784521	18.494861	-0.040853	2.040213
210.586076	1242.885386	18.499866	-0.040818	2.034728
210.475942	1234.919881	18.504871	-0.040792	2.029188
210.608078	1226.972714	18.509875	-0.040812	2.023670
210.418172	1219.074098	18.514880	-0.040772	2.018137
210.395354	1211.139149	18.519885	-0.040762	2.012581
210.501948	1203.199171	18.524890	-0.040777	2.007020
210.493814	1195.260883	18.529895	-0.040771	2.001433
210.282768	1187.391645	18.534899	-0.040727	1.995857
210.002612	1179.480802	18.539904	-0.040670	1.990229
210.119306	1171.521838	18.544909	-0.040686	1.984593
209.922303	1163.652469	18.549914	-0.040645	1.978971
209.743788	1155.740157	18.554919	-0.040607	1.973304
209.745807	1147.801510	18.559923	-0.040602	1.967622
209.705326	1139.872146	18.564928	-0.040590	1.961925
209.604340	1131.972496	18.569933	-0.040566	1.956226
209.869025	1123.980859	18.574938	-0.040610	1.950484
209.636914	1116.059767	18.579943	-0.040562	1.944722
209.441010	1108.186693	18.584947	-0.040521	1.938982
209.595694	1100.238508	18.589952	-0.040545	1.933208
209.542077	1092.308187	18.594957	-0.040530	1.927408
209.429131	1084.420062	18.599962	-0.040504	1.921614
209.311895	1076.522516	18.604967	-0.040477	1.915795
209.476579	1068.576574	18.609971	-0.040503	1.909954
209.338078	1060.684258	18.614976	-0.040472	1.904101
209.090523	1052.804264	18.619981	-0.040421	1.898226
208.986645	1044.903774	18.624986	-0.040397	1.892335
209.254909	1036.930229	18.629991	-0.040442	1.886412
209.009024	1029.078257	18.634995	-0.040391	1.880504
208.864737	1021.192087	18.640000	-0.040359	1.874562
208.808444	1013.255541	18.645005	-0.040344	1.868574
208.970737	1005.322790	18.650010	-0.040369	1.862595
208.566519	997.467912	18.655015	-0.040289	1.856590
208.368184	989.571178	18.660019	-0.040247	1.850557
208.424177	981.642129	18.665024	-0.040253	1.844510
208.287466	973.758418	18.670029	-0.040223	1.838455
208.337006	965.857925	18.675034	-0.040227	1.832389
208.253643	957.927378	18.680039	-0.040206	1.826263
208.174798	950.049359	18.685043	-0.040187	1.820159
208.269032	942.141374	18.690048	-0.040199	1.814031
208.320265	934.217413	18.695053	-0.040204	1.807865
207.980719	926.380860	18.700058	-0.040136	1.801699
207.878888	918.501988	18.705063	-0.040112	1.795507
208.065300	910.512176	18.710067	-0.040142	1.789242
207.908895	902.637703	18.715072	-0.040108	1.783003
207.637275	894.784421	18.720077	-0.040052	1.776746
207.577597	886.894276	18.725082	-0.040036	1.770463
207.563691	878.980698	18.730087	-0.040029	1.764145
207.524632	871.127954	18.735091	-0.040017	1.757849
207.543242	863.228225	18.740096	-0.040015	1.751501
207.326439	855.349486	18.745101	-0.039970	1.745116
207.482323	847.462521	18.750106	-0.039994	1.738749
207.142722	839.615435	18.755111	-0.039926	1.732327
207.340915	831.691503	18.760115	-0.039958	1.725888
207.415690	823.815540	18.765120	-0.039967	1.719448
207.296627	815.949616	18.770125	-0.039940	1.712967
207.328850	808.049082	18.775130	-0.039941	1.706453
206.839085	800.230705	18.780135	-0.039845	1.699913
206.676338	792.387058	18.785139	-0.039810	1.693370
206.832873	784.459872	18.790144	-0.039834	1.686774
206.808010	776.585510	18.795149	-0.039825	1.680172
206.886806	768.728406	18.800154	-0.039834	1.673573
206.561443	760.877955	18.805159	-0.039769	1.666898
206.448268	753.025309	18.810163	-0.039743	1.660224
206.629391	745.135510	18.815168	-0.039772	1.653531
206.360538	737.281121	18.820173	-0.039717	1.646779
206.215113	729.447271	18.825178	-0.039685	1.640035
206.241485	721.564083	18.830183	-0.039685	1.633243
206.240692	713.654224	18.835187	-0.039680	1.626397
205.951479	705.834522	18.840192	-0.039621	1.619559
205.732471	698.002029	18.845197	-0.039576	1.612692
205.889481	690.115371	18.850202	-0.039600	1.605800
205.651851	682.300069	18.855207	-0.039551	1.598885
205.888258	674.416099	18.860211	-0.039590	1.591947
205.643741	666.592392	18.865216	-0.039540	1.584964
205.712878	658.736732	18.870221	-0.039548	1.577966
205.514351	650.916899	18.875226	-0.039506	1.570931
205.436089	643.066951	18.880231	-0.039486	1.563854
205.287731	635.270082	18.885235	-0.039454	1.556782
205.431246	627.376577	18.890240	-0.039476	1.549634
205.259556	619.550561	18.895245	-0.039439	1.542467
205.262985	611.729200	18.900250	-0.039435	1.535297
205.017626	603.910157	18.905255	-0.039384	1.528058
204.893958	596.102667	18.910259	-0.039356	1.520814
204.700557	588.307951	18.915264	-0.039315	1.513537
204.627864	580.461345	18.920269	-0.039297	1.506194
204.561442	572.656611	18.925274	-0.039280	1.498855
204.714250	564.791539	18.930279	-0.039303	1.491457
204.894222	556.949928	18.935283	-0.039332	1.484049
204.399557	549.229104	18.940288	-0.039235	1.476614
204.367914	541.353053	18.945293	-0.039224	1.469064
204.657639	533.494074	18.950298	-0.039273	1.461543
204.226941	525.761040	18.955303	-0.039188	1.453991
204.153323	517.957662	18.960307	-0.039170	1.446387
203.950499	510.198123	18.965312	-0.039127	1.438765
203.880493	502.395862	18.970317	-0.039109	1.431083
203.938552	494.587549	18.975322	-0.039115	1.423373
203.624735	486.836478	18.980327	-0.039052	1.415618
203.758544	479.014034	18.985331	-0.039072	1.407822
203.447082	471.282396	18.990336	-0.039009	1.400000
203.563733	463.466996	18.995341	-0.039026	1.392121
203.630441	455.665262	19.000346	-0.039034	1.384203
203.464538	447.910850	19.005351	-0.038998	1.376248
203.287555	440.156277	19.010355	-0.038960	1.368245
203.114212	432.416772	19.015360	-0.038923	1.360211
202.995224	424.664355	19.020365	-0.038896	1.352125
203.024111	416.889766	19.025370	-0.038897	1.343993
202.888502	409.147950	19.030375	-0.038867	1.335817
202.915780	401.384000	19.035379	-0.038867	1.327596
202.673790	393.680383	19.040384	-0.038817	1.319340
202.485344	385.881011	19.045389	-0.038777	1.310939
202.505835	378.080290	19.050394	-0.038776	1.302520
202.294846	370.378113	19.055399	-0.038732	1.294111
202.313043	362.641184	19.060403	-0.038731	1.285651
202.132328	354.964624	19.065408	-0.038692	1.277165
202.170150	347.223430	19.070413	-0.038695	1.268591
202.199827	339.515284	19.075418	-0.038695	1.259994
202.038105	331.823837	19.080423	-0.038661	1.251321
202.104434	324.119056	19.085427	-0.038668	1.242615
202.050996	316.437281	19.090432	-0.038653	1.233852
201.894815	308.742220	19.095437	-0.038620	1.224990
201.919140	301.065902	19.100442	-0.038619	1.216121
201.673042	293.409578	19.105447	-0.038569	1.207156
201.639631	285.750778	19.110451	-0.038558	1.198164
201.704967	278.067623	19.115456	-0.038565	1.189095
201.493612	270.436421	19.120461	-0.038521	1.179962
201.329604	262.814435	19.125466	-0.038486	1.170778
201.128420	255.188805	19.130471	-0.038444	1.161510
201.237420	247.523063	19.135475	-0.038459	1.152182
201.091129	239.880569	19.140480	-0.038427	1.142754
200.974931	232.270339	19.145485	-0.038401	1.133293
200.856610	224.667886	19.150490	-0.038374	1.123762
200.729385	217.079253	19.155495	-0.038346	1.114165
200.544401	209.503385	19.160499	-0.038307	1.104489
200.419157	201.929166	19.165504	-0.038279	1.094742
200.610817	194.296035	19.170509	-0.038310	1.084901
200.480786	186.760767	19.175514	-0.038281	1.075027
200.198238	179.215030	19.180519	-0.038223	1.065012
200.161127	171.670022	19.185523	-0.038212	1.054959
200.015589	164.141797	19.190528	-0.038180	1.044807
199.838704	156.639685	19.195533	-0.038143	1.034584
199.838641	149.116105	19.200538	-0.038138	1.024271
199.706617	141.622409	19.205543	-0.038109	1.013863
199.592048	134.141841	19.210547	-0.038083	1.003369
199.422812	126.677593	19.215552	-0.038047	0.992774
199.394638	119.168866	19.220557	-0.038037	0.982037
199.051883	111.774064	19.225562	-0.037968	0.971266
198.697178	104.372693	19.230567	-0.037898	0.960362
198.690487	96.938914	19.235571	-0.037892	0.949374
198.788692	89.498339	19.240576	-0.037905	0.938275
198.572438	82.121495	19.245581	-0.037861	0.927057
198.626280	74.739464	19.250586	-0.037866	0.915765
198.382713	67.393065	19.255591	-0.037816	0.904308
198.306893	60.290001	19.260595	-0.037798	0.893134