Thu Mar 11 19:12:45 2021

Number of Points = 3617
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.787689	0.150404	0.000000	0.000088	0.724589

0.903993	0.133445	0.005005	0.000066	0.724596
0.931641	0.127166	0.010010	0.000061	0.724594
0.928312	0.130509	0.015014	0.000061	0.724600
0.689268	0.168000	0.020019	0.000105	0.724590
1.025270	0.111371	0.025024	0.000043	0.724597
0.803943	0.054121	0.030029	0.000084	0.724408
1.177696	-0.087524	0.035034	0.000014	0.724261
1.208223	-0.089253	0.040038	0.000008	0.724269
0.963846	-0.050291	0.045043	0.000053	0.724261
0.897711	-0.035090	0.050048	0.000066	0.724268
0.870254	-0.032076	0.055053	0.000070	0.724264
0.786345	-0.018494	0.060058	0.000086	0.724262
0.839792	-0.026496	0.065062	0.000076	0.724266
1.007517	-0.059388	0.070067	0.000044	0.724260
1.012428	-0.055480	0.075072	0.000043	0.724270
0.739747	-0.010721	0.080077	0.000094	0.724263
0.507524	0.029545	0.085082	0.000137	0.724261
0.845405	-0.028738	0.090086	0.000074	0.724265
0.899848	-0.196322	0.095091	0.000063	0.723956
0.528821	-0.129908	0.100096	0.000132	0.723957
0.667123	-0.154692	0.105101	0.000106	0.723957
0.906422	-0.200405	0.110106	0.000061	0.723952
1.113000	-0.231607	0.115110	0.000023	0.723963
0.912998	-0.201738	0.120115	0.000060	0.723952
0.893098	-0.272018	0.125120	0.000063	0.723808
0.859663	-0.353692	0.130125	0.000069	0.723637
1.187766	-0.414061	0.135130	0.000008	0.723633
1.305167	-0.430066	0.140134	-0.000014	0.723643
0.855023	-0.354145	0.145139	0.000070	0.723635
0.564720	-0.410330	0.150144	0.000124	0.723424
0.714736	-0.476414	0.155149	0.000095	0.723347
0.722084	-0.480949	0.160154	0.000094	0.723341
0.549571	-0.446254	0.165158	0.000126	0.723350
0.265060	-0.427605	0.170163	0.000179	0.723287
0.780559	-0.659757	0.175168	0.000083	0.723012
0.589170	-0.626001	0.180173	0.000118	0.723012
0.402249	-0.594711	0.185178	0.000152	0.723009
0.583394	-0.660984	0.190182	0.000119	0.722942
0.771062	-0.822054	0.195187	0.000084	0.722692
0.766912	-0.817022	0.200192	0.000084	0.722701
0.566082	-0.782378	0.205197	0.000121	0.722699
0.587330	-0.924986	0.210202	0.000117	0.722427
0.733555	-0.975395	0.215206	0.000090	0.722380
0.500069	-0.939071	0.220211	0.000133	0.722370
0.616834	-1.056576	0.225216	0.000111	0.722180
0.525142	-1.091995	0.230221	0.000128	0.722079
0.266841	-1.049461	0.235226	0.000176	0.722073
0.257374	-1.140276	0.240230	0.000178	0.721891
0.205795	-1.205498	0.245235	0.000187	0.721746
0.073437	-1.178238	0.250240	0.000211	0.721753
0.194682	-1.296855	0.255245	0.000189	0.721563
0.320072	-1.383510	0.260250	0.000165	0.721437
-0.131830	-1.300144	0.265254	0.000249	0.721443
-0.384270	-1.385477	0.270259	0.000296	0.721187
0.547392	-1.582975	0.275264	0.000122	0.721125
0.612050	-1.621715	0.280269	0.000110	0.721072
-0.275070	-1.564168	0.285274	0.000275	0.720875
-0.454960	-1.526979	0.290278	0.000308	0.720886
-0.251276	-1.658494	0.295283	0.000270	0.720699
-0.077313	-1.766929	0.300288	0.000238	0.720547
-0.518152	-1.693145	0.305293	0.000320	0.720538
-1.239565	-1.725236	0.310298	0.000454	0.720222
-1.433536	-1.686494	0.315302	0.000490	0.720231
-1.561914	-1.685592	0.320307	0.000513	0.720188
-2.333555	-1.694391	0.325312	0.000657	0.719900
-2.680091	-1.633670	0.330317	0.000721	0.719899
-3.038492	-1.572500	0.335322	0.000787	0.719894
-2.793821	-1.713200	0.340326	0.000742	0.719703
-3.886619	-1.572879	0.345331	0.000945	0.719596
-3.467954	-1.643918	0.350336	0.000867	0.719604
-3.274955	-1.679164	0.355341	0.000831	0.719602
-4.240533	-1.668255	0.360346	0.001010	0.719285
-4.725540	-1.587659	0.365350	0.001100	0.719274
-4.792344	-1.580988	0.370355	0.001113	0.719264
-4.340082	-1.659638	0.375360	0.001028	0.719268
-4.711521	-1.676675	0.380365	0.001097	0.719105
-6.195185	-1.486901	0.385370	0.001373	0.718958
-5.241756	-1.653387	0.390374	0.001195	0.718965
-5.469156	-1.618349	0.395379	0.001238	0.718955
-5.920701	-1.535083	0.400384	0.001321	0.718961
-5.494751	-1.692436	0.405389	0.001242	0.718800
-6.752530	-1.549419	0.410394	0.001476	0.718641
-6.494778	-1.591532	0.415398	0.001428	0.718649
-6.593450	-1.580328	0.420403	0.001446	0.718637
-6.377347	-1.617001	0.425408	0.001405	0.718641
-6.535750	-1.605201	0.430413	0.001435	0.718609
-7.391564	-1.583913	0.435418	0.001594	0.718350
-7.115655	-1.629381	0.440422	0.001542	0.718358
-7.744945	-1.521809	0.445427	0.001659	0.718349
-7.578032	-1.548102	0.450432	0.001628	0.718356
-6.893594	-1.670799	0.455437	0.001500	0.718355
-7.343684	-1.652373	0.460442	0.001584	0.718234
-8.601297	-1.534160	0.465446	0.001818	0.718025
-8.375462	-1.578733	0.470451	0.001776	0.718017
-8.313038	-1.590052	0.475456	0.001764	0.718017
-8.414941	-1.571036	0.480461	0.001783	0.718019
-8.730808	-1.517703	0.485466	0.001841	0.718014
-8.058142	-1.633012	0.490470	0.001716	0.718023
-8.682642	-1.673223	0.495475	0.001832	0.717724
-9.535567	-1.531258	0.500480	0.001990	0.717705
-9.660683	-1.508187	0.505485	0.002013	0.717707
-9.084049	-1.613623	0.510490	0.001906	0.717702
-9.292807	-1.573639	0.515494	0.001944	0.717708
-9.574843	-1.526566	0.520499	0.001997	0.717702
-9.173040	-1.626489	0.525504	0.001922	0.717646
-10.198468	-1.575229	0.530509	0.002113	0.717387
-10.432644	-1.538257	0.535514	0.002156	0.717378
-10.292057	-1.558842	0.540518	0.002129	0.717387
-10.204965	-1.579331	0.545523	0.002113	0.717378
-10.461790	-1.531655	0.550528	0.002161	0.717382
-10.163355	-1.584263	0.555533	0.002105	0.717383
-9.987676	-1.649462	0.560538	0.002072	0.717317
-11.177700	-1.550234	0.565542	0.002293	0.717094
-11.431034	-1.511267	0.570547	0.002340	0.717082
-11.111250	-1.567640	0.575552	0.002281	0.717084
-10.927490	-1.600849	0.580557	0.002246	0.717083
-11.538904	-1.494154	0.585562	0.002360	0.717079
-11.392763	-1.514823	0.590566	0.002332	0.717090
-10.935957	-1.602389	0.595571	0.002247	0.717078
-11.868941	-1.598002	0.600576	0.002421	0.716759
-12.231067	-1.533659	0.605581	0.002488	0.716759
-12.384608	-1.509467	0.610586	0.002516	0.716753
-11.994765	-1.574772	0.615590	0.002443	0.716762
-12.327113	-1.519794	0.620595	0.002505	0.716754
-12.261963	-1.528761	0.625600	0.002493	0.716759
-11.797259	-1.609688	0.630605	0.002406	0.716763
-12.660809	-1.569146	0.635610	0.002567	0.716539
-13.260355	-1.505555	0.640614	0.002678	0.716454
-12.915571	-1.572375	0.645619	0.002614	0.716444
-13.293050	-1.502063	0.650624	0.002684	0.716450
-13.186749	-1.519268	0.655629	0.002664	0.716454
-12.946514	-1.565101	0.660634	0.002619	0.716449
-12.795535	-1.588963	0.665638	0.002590	0.716455
-13.552107	-1.493375	0.670643	0.002731	0.716378
-13.838410	-1.566189	0.675648	0.002784	0.716133
-13.424945	-1.639137	0.680653	0.002707	0.716135
-14.491814	-1.453703	0.685658	0.002905	0.716126
-13.973928	-1.540957	0.690662	0.002809	0.716136
-13.811668	-1.573174	0.695667	0.002778	0.716130
-14.192330	-1.503911	0.700672	0.002849	0.716133
-14.262331	-1.491011	0.705677	0.002862	0.716135
-14.506453	-1.568893	0.710682	0.002907	0.715895
-14.613969	-1.552776	0.715686	0.002927	0.715889
-15.131040	-1.464569	0.720691	0.003023	0.715882
-14.698518	-1.540637	0.725696	0.002942	0.715884
-14.503587	-1.574893	0.730701	0.002906	0.715885
-14.874995	-1.512082	0.735706	0.002975	0.715879
-14.359660	-1.632085	0.740710	0.002879	0.715824
-15.451484	-1.581142	0.745715	0.003082	0.715539
-15.752795	-1.524753	0.750720	0.003137	0.715545
-15.780462	-1.518647	0.755725	0.003142	0.715548
-15.835530	-1.511478	0.760730	0.003152	0.715543
-15.564848	-1.557734	0.765734	0.003102	0.715547
-15.897438	-1.503056	0.770739	0.003164	0.715539
-15.722619	-1.538729	0.775744	0.003131	0.715530
-15.857595	-1.664592	0.780749	0.003156	0.715233
-16.649041	-1.525923	0.785754	0.003303	0.715229
-17.067078	-1.447284	0.790758	0.003380	0.715238
-16.231665	-1.601978	0.795763	0.003225	0.715226
-16.214616	-1.602855	0.800768	0.003221	0.715231
-16.618706	-1.528038	0.805773	0.003296	0.715237
-16.478655	-1.602526	0.810778	0.003270	0.715139
-17.249844	-1.579646	0.815782	0.003414	0.714912
-17.375230	-1.562622	0.820787	0.003437	0.714902
-17.616686	-1.516936	0.825792	0.003481	0.714908
-17.312980	-1.570849	0.830797	0.003425	0.714909
-17.548345	-1.531832	0.835802	0.003468	0.714903
-17.658135	-1.507912	0.840806	0.003488	0.714912
-17.391911	-1.578861	0.845811	0.003439	0.714866
-18.104371	-1.582710	0.850816	0.003571	0.714607
-18.279671	-1.549046	0.855821	0.003604	0.714612
-18.406333	-1.527821	0.860826	0.003627	0.714610
-18.091148	-1.581972	0.865830	0.003568	0.714614
-18.579838	-1.499788	0.870835	0.003659	0.714605
-18.480040	-1.515292	0.875840	0.003640	0.714610
-17.956999	-1.635405	0.880845	0.003542	0.714557
-19.358924	-1.529010	0.885850	0.003803	0.714273
-19.381417	-1.520999	0.890854	0.003807	0.714281
-19.370747	-1.526952	0.895859	0.003805	0.714273
-18.936627	-1.602923	0.900864	0.003724	0.714276
-19.228128	-1.549069	0.905869	0.003778	0.714281
-19.496920	-1.504957	0.910874	0.003828	0.714273
-19.332433	-1.529551	0.915878	0.003797	0.714283
-19.811380	-1.573117	0.920883	0.003886	0.714028
-20.595831	-1.461640	0.925888	0.004032	0.713972
-20.185605	-1.533593	0.930893	0.003955	0.713974
-20.200441	-1.535117	0.935898	0.003958	0.713966
-20.364756	-1.502508	0.940902	0.003988	0.713974
-20.405950	-1.498983	0.945907	0.003996	0.713966
-20.500325	-1.479502	0.950912	0.004013	0.713972
-20.517572	-1.475373	0.955917	0.004016	0.713975
-21.034738	-1.542572	0.960922	0.004112	0.713658
-20.910742	-1.565846	0.965926	0.004089	0.713656
-21.387420	-1.487242	0.970931	0.004177	0.713644
-21.495300	-1.465435	0.975936	0.004197	0.713650
-20.986176	-1.554029	0.980941	0.004102	0.713654
-20.996652	-1.558762	0.985946	0.004104	0.713641
-21.216623	-1.513019	0.990950	0.004145	0.713655
-21.453943	-1.561840	0.995955	0.004189	0.713474
-21.840157	-1.552091	1.000960	0.004260	0.713357
-21.711490	-1.573019	1.005965	0.004236	0.713361
-22.322255	-1.469226	1.010970	0.004350	0.713352
-22.210187	-1.486451	1.015974	0.004329	0.713358
-21.890541	-1.546546	1.020979	0.004269	0.713352
-22.189107	-1.491393	1.025984	0.004324	0.713356
-22.169801	-1.588015	1.030989	0.004321	0.713171
-23.356190	-1.455082	1.035994	0.004541	0.713015
-22.897537	-1.532336	1.040998	0.004456	0.713025
-22.894390	-1.536235	1.046003	0.004455	0.713018
-23.086875	-1.499865	1.051008	0.004490	0.713023
-23.048850	-1.506056	1.056013	0.004483	0.713025
-23.074112	-1.504031	1.061018	0.004488	0.713020
-22.750563	-1.604273	1.066022	0.004427	0.712936
-23.983061	-1.499238	1.071027	0.004656	0.712708
-24.214334	-1.456858	1.076032	0.004699	0.712711
-24.060181	-1.484683	1.081037	0.004670	0.712710
-23.824520	-1.528990	1.086042	0.004626	0.712706
-23.863312	-1.518202	1.091046	0.004633	0.712714
-24.272351	-1.448539	1.096051	0.004709	0.712708
-23.963640	-1.501786	1.101056	0.004652	0.712712
-23.800116	-1.640438	1.106061	0.004621	0.712495
-25.051905	-1.473940	1.111066	0.004854	0.712382
-24.771033	-1.518036	1.116070	0.004801	0.712395
-24.588867	-1.556181	1.121075	0.004767	0.712384
-24.861230	-1.507107	1.126080	0.004818	0.712385
-24.818880	-1.512973	1.131085	0.004810	0.712389
-24.801316	-1.518968	1.136090	0.004806	0.712384
-25.182814	-1.540985	1.141094	0.004877	0.712205
-26.034576	-1.446207	1.146099	0.005035	0.712091
-25.506846	-1.538915	1.151104	0.004937	0.712095
-25.549745	-1.530923	1.156109	0.004945	0.712096
-25.854886	-1.481491	1.161114	0.005001	0.712086
-25.465926	-1.545085	1.166118	0.004929	0.712098
-25.700485	-1.506428	1.171123	0.004972	0.712092
-26.048660	-1.515117	1.176128	0.005037	0.711952
-26.774436	-1.479290	1.181133	0.005172	0.711766
-26.354683	-1.558123	1.186138	0.005093	0.711758
-26.602016	-1.509985	1.191142	0.005139	0.711766
-27.071054	-1.429739	1.196147	0.005226	0.711760
-26.674200	-1.500538	1.201152	0.005152	0.711760
-26.453548	-1.537043	1.206157	0.005111	0.711766
-26.875522	-1.466828	1.211162	0.005189	0.711757
-27.254879	-1.547603	1.216166	0.005260	0.711461
-27.477645	-1.513664	1.221171	0.005301	0.711450
-27.668497	-1.477078	1.226176	0.005336	0.711456
-27.414388	-1.520603	1.231181	0.005289	0.711460
-27.778692	-1.459800	1.236186	0.005356	0.711452
-27.671137	-1.476036	1.241190	0.005336	0.711458
-27.589165	-1.493231	1.246195	0.005321	0.711453
-27.805848	-1.555051	1.251200	0.005361	0.711253
-28.602608	-1.468265	1.256205	0.005509	0.711144
-28.603943	-1.472373	1.261210	0.005509	0.711135
-28.439279	-1.498827	1.266214	0.005478	0.711142
-28.511561	-1.488259	1.271219	0.005491	0.711137
-28.916771	-1.415235	1.276224	0.005566	0.711139
-28.815933	-1.432349	1.281229	0.005548	0.711142
-28.770659	-1.444568	1.286234	0.005539	0.711134
-28.551173	-1.602715	1.291238	0.005498	0.710896
-29.505730	-1.446964	1.296243	0.005675	0.710868
-29.273807	-1.488924	1.301248	0.005632	0.710867
-28.559531	-1.613791	1.306253	0.005499	0.710873
-29.066901	-1.530576	1.311258	0.005593	0.710859
-29.167018	-1.506250	1.316262	0.005611	0.710872
-29.256715	-1.587682	1.321267	0.005628	0.710678
-30.309421	-1.474262	1.326272	0.005824	0.710530
-30.011974	-1.524109	1.331277	0.005768	0.710537
-30.109939	-1.512166	1.336282	0.005786	0.710526
-30.087924	-1.512656	1.341286	0.005782	0.710533
-30.020146	-1.527592	1.346291	0.005769	0.710528
-30.050690	-1.520162	1.351296	0.005775	0.710533
-30.491081	-1.572524	1.356301	0.005856	0.710272
-31.410603	-1.438737	1.361306	0.006027	0.710212
-31.168801	-1.480389	1.366310	0.005982	0.710215
-30.505273	-1.601922	1.371315	0.005858	0.710209
-30.994737	-1.511927	1.376320	0.005949	0.710215
-31.032992	-1.503163	1.381325	0.005956	0.710219
-30.825930	-1.545146	1.386330	0.005917	0.710209
-31.072263	-1.639759	1.391334	0.005963	0.709933
-31.966813	-1.501932	1.396339	0.006129	0.709890
-32.288022	-1.443796	1.401344	0.006189	0.709892
-31.423536	-1.597318	1.406349	0.006028	0.709894
-31.844952	-1.526360	1.411354	0.006106	0.709886
-31.786311	-1.533615	1.416358	0.006095	0.709893
-31.790575	-1.545938	1.421363	0.006096	0.709867
-32.434498	-1.567320	1.426368	0.006215	0.709595
-32.577411	-1.540646	1.431373	0.006242	0.709598
-32.944391	-1.478879	1.436378	0.006310	0.709591
-32.491835	-1.556533	1.441382	0.006225	0.709597
-32.543164	-1.548991	1.446387	0.006235	0.709595
-33.118546	-1.446961	1.451392	0.006342	0.709594
-32.417607	-1.604975	1.456397	0.006211	0.709528
-33.727779	-1.506728	1.461402	0.006455	0.709258
-33.470848	-1.548078	1.466406	0.006407	0.709267
-33.658821	-1.518171	1.471411	0.006441	0.709261
-33.743196	-1.500604	1.476416	0.006457	0.709266
-33.887305	-1.472899	1.481421	0.006483	0.709270
-34.035948	-1.452263	1.486426	0.006511	0.709259
-33.605582	-1.523275	1.491430	0.006431	0.709271
-33.990051	-1.579116	1.496435	0.006502	0.709022
-35.034005	-1.426747	1.501440	0.006696	0.708955
-34.264061	-1.561833	1.506445	0.006553	0.708960
-34.363527	-1.548594	1.511450	0.006571	0.708951
-34.902836	-1.448466	1.516454	0.006671	0.708960
-34.711744	-1.484479	1.521459	0.006635	0.708956
-34.367745	-1.545911	1.526464	0.006571	0.708957
-34.823077	-1.552819	1.531469	0.006656	0.708781
-36.009161	-1.414421	1.536474	0.006876	0.708635
-35.448984	-1.510215	1.541478	0.006772	0.708643
-35.270769	-1.543192	1.546483	0.006738	0.708641
-35.816049	-1.446675	1.551488	0.006840	0.708640
-35.215708	-1.552394	1.556493	0.006728	0.708643
-35.555610	-1.494820	1.561498	0.006791	0.708638
-35.690869	-1.498695	1.566502	0.006816	0.708582
-36.134358	-1.538667	1.571507	0.006898	0.708344
-36.154649	-1.533927	1.576512	0.006902	0.708347
-36.623843	-1.448438	1.581517	0.006989	0.708351
-36.515045	-1.471964	1.586522	0.006968	0.708343
-35.870760	-1.582986	1.591526	0.006848	0.708351
-36.165878	-1.532534	1.596531	0.006903	0.708347
-36.695408	-1.496228	1.601536	0.007001	0.708231
-37.290592	-1.499834	1.606541	0.007112	0.708012
-37.100683	-1.536492	1.611546	0.007076	0.708006
-37.497110	-1.462570	1.616550	0.007150	0.708013
-37.361953	-1.490637	1.621555	0.007125	0.708006
-37.083575	-1.541545	1.626560	0.007073	0.708004
-36.867384	-1.574946	1.631565	0.007032	0.708014
-37.355722	-1.525283	1.636570	0.007123	0.707940
-37.981634	-1.532585	1.641574	0.007239	0.707702
-38.020805	-1.529423	1.646579	0.007246	0.707694
-38.378083	-1.465241	1.651584	0.007312	0.707696
-37.856537	-1.556107	1.656589	0.007215	0.707700
-38.053699	-1.525329	1.661594	0.007252	0.707692
-38.323019	-1.473479	1.666598	0.007302	0.707700
-38.220133	-1.503887	1.671603	0.007282	0.707676
-38.521081	-1.601891	1.676608	0.007338	0.707373
-39.016170	-1.510422	1.681613	0.007430	0.707379
-39.460711	-1.435391	1.686618	0.007513	0.707371
-38.840243	-1.541054	1.691622	0.007397	0.707382
-38.939274	-1.525703	1.696627	0.007415	0.707377
-39.488852	-1.429850	1.701632	0.007517	0.707374
-39.065086	-1.502162	1.706637	0.007438	0.707381
-39.143580	-1.611642	1.711642	0.007453	0.707133
-40.039048	-1.475204	1.716646	0.007619	0.707087
-40.152406	-1.459009	1.721651	0.007640	0.707079
-39.615966	-1.555607	1.726656	0.007540	0.707078
-39.626190	-1.550020	1.731661	0.007542	0.707086
-40.261247	-1.443437	1.736666	0.007660	0.707073
-40.022804	-1.482369	1.741670	0.007615	0.707080
-40.112262	-1.600177	1.746675	0.007631	0.706812
-40.871412	-1.498126	1.751680	0.007773	0.706746
-40.671970	-1.530187	1.756685	0.007735	0.706753
-40.554440	-1.554679	1.761690	0.007713	0.706747
-40.771475	-1.513201	1.766694	0.007753	0.706753
-40.626739	-1.540562	1.771699	0.007726	0.706750
-40.674576	-1.548244	1.776704	0.007735	0.706718
-41.088262	-1.609777	1.781709	0.007812	0.706446
-41.740956	-1.496116	1.786714	0.007933	0.706441
-41.700225	-1.499772	1.791718	0.007925	0.706449
-41.253843	-1.581640	1.796723	0.007842	0.706445
-41.623095	-1.517146	1.801728	0.007910	0.706442
-41.805796	-1.482565	1.806733	0.007944	0.706447
-41.524053	-1.573108	1.811738	0.007892	0.706366
-42.220030	-1.565226	1.816742	0.008021	0.706133
-42.334707	-1.546615	1.821747	0.008042	0.706130
-42.662746	-1.490357	1.826752	0.008103	0.706126
-42.189622	-1.570472	1.831757	0.008015	0.706135
-42.739729	-1.476726	1.836762	0.008117	0.706126
-42.739962	-1.474866	1.841766	0.008117	0.706130
-42.407034	-1.567334	1.846771	0.008055	0.706064
-43.225158	-1.522644	1.851776	0.008207	0.705861
-43.086260	-1.544695	1.856781	0.008181	0.705867
-43.414029	-1.490774	1.861786	0.008241	0.705858
-43.184445	-1.528641	1.866790	0.008198	0.705865
-43.071406	-1.550196	1.871795	0.008177	0.705863
-43.357336	-1.499542	1.876800	0.008230	0.705862
-43.040941	-1.655048	1.881805	0.008171	0.705663
-44.274391	-1.504529	1.886810	0.008401	0.705524
-43.944632	-1.561848	1.891814	0.008339	0.705528
-43.756378	-1.595415	1.896819	0.008304	0.705528
-44.344891	-1.491478	1.901824	0.008413	0.705526
-44.415480	-1.476302	1.906829	0.008426	0.705532
-44.088378	-1.539974	1.911834	0.008365	0.705522
-44.341209	-1.624858	1.916838	0.008412	0.705261
-45.323217	-1.472636	1.921843	0.008594	0.705215
-45.411240	-1.458657	1.926848	0.008611	0.705212
-44.477623	-1.621690	1.931853	0.008437	0.705219
-45.141648	-1.508631	1.936858	0.008560	0.705209
-45.379533	-1.464563	1.941862	0.008604	0.705213
-44.889300	-1.552508	1.946867	0.008513	0.705212
-45.384067	-1.595092	1.951872	0.008604	0.704949
-46.035812	-1.507624	1.956877	0.008726	0.704892
-46.005732	-1.516365	1.961882	0.008720	0.704885
-45.779282	-1.553371	1.966886	0.008677	0.704892
-45.975170	-1.520742	1.971891	0.008714	0.704888
-46.135359	-1.493664	1.976896	0.008743	0.704886
-45.599551	-1.585279	1.981901	0.008643	0.704894
-46.454238	-1.556816	1.986906	0.008802	0.704645
-47.062264	-1.472828	1.991910	0.008915	0.704596
-46.506576	-1.573491	1.996915	0.008812	0.704593
-46.693007	-1.540929	2.001920	0.008846	0.704592

-46.676457	-1.545406	2.011917	0.008843	0.704590
-46.923959	-1.501450	2.021914	0.008888	0.704590
-47.382698	-1.568376	2.031910	0.008973	0.704291
-47.770311	-1.513201	2.041907	0.009045	0.704264
-47.677861	-1.514230	2.051904	0.009027	0.704296
-47.240536	-1.477213	2.061901	0.008945	0.704529
-46.760595	-1.532580	2.071898	0.008856	0.704590
-46.659331	-1.550414	2.081894	0.008836	0.704591
-46.844923	-1.516565	2.091891	0.008871	0.704594
-46.700041	-1.542291	2.101888	0.008843	0.704595
-46.843159	-1.519156	2.111885	0.008869	0.704591
-47.061387	-1.480574	2.121882	0.008910	0.704591
-46.862291	-1.516392	2.131878	0.008872	0.704591
-47.015533	-1.488077	2.141875	0.008900	0.704594
-46.210535	-1.530599	2.151872	0.008750	0.704798
-46.170760	-1.493746	2.161869	0.008742	0.704888
-46.324726	-1.466816	2.171866	0.008770	0.704887
-45.722388	-1.574211	2.181862	0.008658	0.704888
-46.091486	-1.465353	2.191859	0.008726	0.704976
-44.972566	-1.545883	2.201856	0.008517	0.705216
-45.229366	-1.501474	2.211853	0.008565	0.705214
-45.287285	-1.491628	2.221850	0.008575	0.705214
-45.194646	-1.462347	2.231846	0.008557	0.705307
-44.317777	-1.510577	2.241843	0.008394	0.705525
-44.186067	-1.535157	2.251840	0.008369	0.705524
-44.329254	-1.510926	2.261837	0.008395	0.705522
-44.153915	-1.460203	2.271834	0.008362	0.705688
-43.299672	-1.528736	2.281830	0.008203	0.705857
-43.636949	-1.467109	2.291827	0.008265	0.705861
-43.208349	-1.545274	2.301824	0.008185	0.705858
-43.068073	-1.461635	2.311821	0.008158	0.706077
-42.555403	-1.531348	2.321818	0.008062	0.706122
-42.623694	-1.516815	2.331814	0.008075	0.706127
-42.660922	-1.451142	2.341811	0.008081	0.706247
-41.572217	-1.548210	2.351808	0.007878	0.706443
-41.880152	-1.494498	2.361805	0.007935	0.706441
-41.874326	-1.497454	2.371802	0.007933	0.706438
-41.242972	-1.465428	2.381798	0.007815	0.706729
-41.023732	-1.496039	2.391795	0.007774	0.706747
-40.870727	-1.521885	2.401792	0.007745	0.706751
-40.869448	-1.426712	2.411789	0.007744	0.706943
-39.980402	-1.518329	2.421786	0.007579	0.707078
-40.214182	-1.476202	2.431782	0.007622	0.707080
-39.728658	-1.555596	2.441779	0.007531	0.707095
-39.244987	-1.503913	2.451776	0.007440	0.707373
-39.235438	-1.506172	2.461773	0.007438	0.707372
-39.276305	-1.497887	2.471770	0.007445	0.707375
-38.874971	-1.475608	2.481766	0.007370	0.707564
-38.329008	-1.506316	2.491763	0.007268	0.707699
-38.082205	-1.550824	2.501760	0.007222	0.707698
-38.441805	-1.478130	2.511757	0.007288	0.707716
-37.330755	-1.530617	2.521754	0.007081	0.708009
-37.476977	-1.504878	2.531750	0.007108	0.708009
-37.425994	-1.513197	2.541747	0.007098	0.708012
-37.087686	-1.472964	2.551744	0.007034	0.708214
-36.525250	-1.508254	2.561741	0.006929	0.708345
-36.553483	-1.503857	2.571738	0.006934	0.708344
-36.566333	-1.496820	2.581734	0.006936	0.708355
-35.948659	-1.466611	2.591731	0.006821	0.708637
-35.571002	-1.533580	2.601728	0.006750	0.708638
-35.826159	-1.489090	2.611725	0.006797	0.708637
-35.293697	-1.482896	2.621722	0.006698	0.708840
-35.112200	-1.459519	2.631718	0.006663	0.708953
-34.779220	-1.516768	2.641715	0.006601	0.708958
-35.039251	-1.418437	2.651712	0.006649	0.709063
-33.907236	-1.521335	2.661709	0.006438	0.709261
-34.133496	-1.481373	2.671706	0.006479	0.709261
-34.219350	-1.466433	2.681702	0.006495	0.709261
-33.162972	-1.492374	2.691699	0.006298	0.709587
-32.979708	-1.521178	2.701696	0.006263	0.709595
-33.003844	-1.518059	2.711693	0.006267	0.709594
-32.900513	-1.501592	2.721690	0.006248	0.709664
-32.341113	-1.488312	2.731686	0.006143	0.709891
-31.995967	-1.548855	2.741683	0.006078	0.709894
-32.529647	-1.452974	2.751680	0.006177	0.709896
-31.482447	-1.503084	2.761677	0.005982	0.710170
-31.512494	-1.474706	2.771674	0.005987	0.710217
-31.442647	-1.486734	2.781670	0.005974	0.710218
-31.156384	-1.480932	2.791667	0.005920	0.710333
-30.361734	-1.522761	2.801664	0.005772	0.710533
-30.406747	-1.515883	2.811661	0.005780	0.710531
-30.460889	-1.506910	2.821658	0.005789	0.710531
-29.683540	-1.530008	2.831654	0.005644	0.710762
-29.474115	-1.513127	2.841651	0.005605	0.710871
-29.646553	-1.483621	2.851648	0.005636	0.710870
-29.266966	-1.549199	2.861645	0.005565	0.710874
-29.167603	-1.438066	2.871642	0.005546	0.711132
-28.657060	-1.528035	2.881638	0.005451	0.711135
-28.725776	-1.514820	2.891635	0.005463	0.711138
-28.179065	-1.497063	2.901632	0.005361	0.711369
-27.817377	-1.519801	2.911629	0.005293	0.711453
-28.236467	-1.446345	2.921626	0.005371	0.711451
-27.685871	-1.495844	2.931622	0.005268	0.711549
-27.020966	-1.507150	2.941619	0.005144	0.711763
-27.085042	-1.497622	2.951616	0.005155	0.711760
-27.110463	-1.494473	2.961613	0.005160	0.711758
-26.639333	-1.416007	2.971610	0.005071	0.712083
-26.082101	-1.514640	2.981606	0.004967	0.712085
-26.088283	-1.512214	2.991603	0.004968	0.712088
-25.932692	-1.448329	3.001600	0.004939	0.712272
-25.285958	-1.508224	3.011597	0.004818	0.712383
-25.393150	-1.489407	3.021594	0.004837	0.712383
-25.066615	-1.527276	3.031590	0.004776	0.712424
-24.636324	-1.463428	3.041587	0.004695	0.712705
-24.311420	-1.520542	3.051584	0.004635	0.712707
-24.745766	-1.444455	3.061581	0.004715	0.712705
-24.004781	-1.452555	3.071578	0.004577	0.712953
-23.539291	-1.502479	3.081574	0.004490	0.713019
-23.367117	-1.533085	3.091571	0.004457	0.713020
-23.583544	-1.454122	3.101568	0.004497	0.713102
-22.502771	-1.520132	3.111565	0.004295	0.713354
-22.923241	-1.447543	3.121562	0.004373	0.713350
-22.602287	-1.501828	3.131558	0.004313	0.713357
-22.265230	-1.452691	3.141555	0.004250	0.713575
-21.875956	-1.483381	3.151552	0.004177	0.713653
-21.892790	-1.482158	3.161549	0.004180	0.713650
-21.855888	-1.438231	3.171546	0.004172	0.713751
-20.890530	-1.501913	3.181542	0.003992	0.713967
-20.967500	-1.486202	3.191539	0.004006	0.713972
-20.845263	-1.508853	3.201536	0.003983	0.713971
-20.233462	-1.485274	3.211533	0.003869	0.714235
-20.117225	-1.484787	3.221530	0.003847	0.714278
-19.878697	-1.527093	3.231526	0.003802	0.714279
-20.134156	-1.434336	3.241523	0.003849	0.714374
-18.903848	-1.533936	3.251520	0.003619	0.714612
-19.160809	-1.488518	3.261517	0.003667	0.714612
-19.027438	-1.514648	3.271514	0.003642	0.714608
-18.598888	-1.503100	3.281510	0.003561	0.714784
-18.188547	-1.514905	3.291507	0.003484	0.714906
-18.125120	-1.526094	3.301504	0.003472	0.714907
-18.264319	-1.500239	3.311501	0.003498	0.714910
-17.608535	-1.461694	3.321498	0.003375	0.715219
-17.365493	-1.500507	3.331494	0.003330	0.715229
-17.502401	-1.473996	3.341491	0.003355	0.715234
-17.017206	-1.466072	3.351488	0.003264	0.715422
-16.777186	-1.447238	3.361485	0.003219	0.715545
-16.377822	-1.518862	3.371482	0.003144	0.715545
-16.597993	-1.452095	3.381478	0.003185	0.715600
-15.826602	-1.447862	3.391475	0.003040	0.715881
-15.550739	-1.495946	3.401472	0.002989	0.715884
-15.645683	-1.479710	3.411469	0.003006	0.715884
-15.245996	-1.467779	3.421466	0.002931	0.716049
-15.107465	-1.452425	3.431462	0.002905	0.716129
-15.005100	-1.469168	3.441459	0.002885	0.716133
-14.638356	-1.458637	3.451456	0.002817	0.716284
-14.067028	-1.478295	3.461453	0.002710	0.716448
-13.894492	-1.509470	3.471450	0.002677	0.716448
-14.081969	-1.471976	3.481446	0.002712	0.716457
-13.335854	-1.454407	3.491443	0.002572	0.716755
-13.139844	-1.489288	3.501440	0.002536	0.716756
-13.270019	-1.467212	3.511437	0.002559	0.716755
-12.809476	-1.439430	3.521434	0.002473	0.716973
-12.394480	-1.455924	3.531430	0.002396	0.717087
-12.347863	-1.464826	3.541427	0.002386	0.717087
-12.135691	-1.458497	3.551424	0.002347	0.717175
-11.556014	-1.458504	3.561421	0.002238	0.717380
-11.380729	-1.491115	3.571418	0.002205	0.717378
-11.266110	-1.511497	3.581414	0.002183	0.717379
-10.837863	-1.471809	3.591411	0.002103	0.717609
-10.571746	-1.470862	3.601408	0.002053	0.717705
-10.471380	-1.488665	3.611405	0.002034	0.717706
-10.433972	-1.473942	3.621402	0.002027	0.717749
-9.875586	-1.438541	3.631398	0.001922	0.718016
-9.468774	-1.512072	3.641395	0.001846	0.718015
-9.762701	-1.460319	3.651392	0.001900	0.718015
-9.207749	-1.435846	3.661389	0.001797	0.718259
-8.777879	-1.466628	3.671386	0.001716	0.718350
-8.813508	-1.460010	3.681382	0.001722	0.718352
-8.588873	-1.466502	3.691379	0.001680	0.718419
-8.041582	-1.449972	3.701376	0.001578	0.718644
-7.930846	-1.471560	3.711373	0.001557	0.718642
-7.885413	-1.480132	3.721370	0.001548	0.718641
-7.503620	-1.420820	3.731366	0.001476	0.718893
-6.915580	-1.491847	3.741363	0.001367	0.718961
-7.057518	-1.466177	3.751360	0.001393	0.718962
-6.984468	-1.435378	3.761357	0.001379	0.719050
-6.413622	-1.425709	3.771354	0.001272	0.719270
-5.883436	-1.518949	3.781350	0.001173	0.719273
-6.074806	-1.485584	3.791347	0.001208	0.719272
-5.500287	-1.457263	3.801344	0.001101	0.719531
-5.048281	-1.500697	3.811341	0.001016	0.719605
-5.080415	-1.496762	3.821338	0.001022	0.719602
-5.015191	-1.507946	3.831334	0.001009	0.719604
-4.681451	-1.417442	3.841331	0.000946	0.719900
-4.402616	-1.466389	3.851328	0.000894	0.719902
-4.406855	-1.465480	3.861325	0.000894	0.719903
-4.465367	-1.343902	3.871322	0.000905	0.720123
-3.658436	-1.436777	3.881318	0.000754	0.720224
-3.683988	-1.430921	3.891315	0.000759	0.720227
-3.276180	-1.430045	3.901312	0.000682	0.720373
-2.753041	-1.439248	3.911309	0.000584	0.720539
-3.330031	-1.337375	3.921306	0.000691	0.720538
-2.736890	-1.395042	3.931302	0.000580	0.720633
-2.589679	-1.295563	3.941299	0.000553	0.720881
-2.273363	-1.353205	3.951296	0.000493	0.720879
-1.761583	-1.424562	3.961293	0.000398	0.720919
-2.544164	-1.182228	3.971290	0.000543	0.721122
-1.279975	-1.405720	3.981286	0.000307	0.721126
-1.944040	-1.219040	3.991283	0.000430	0.721262
-1.619856	-1.186462	4.001280	0.000369	0.721440
-1.289730	-1.242746	4.011277	0.000308	0.721446
-1.623171	-1.032636	4.021274	0.000369	0.721743
-1.004021	-1.141814	4.031270	0.000253	0.721746
-1.360162	-0.942917	4.041267	0.000319	0.722013
-0.504588	-1.061644	4.051264	0.000160	0.722079
-0.580401	-0.950690	4.061261	0.000173	0.722272
-0.663819	-0.887478	4.071258	0.000188	0.722367
-0.805622	-0.747893	4.081254	0.000214	0.722593
-0.833913	-0.691529	4.091251	0.000219	0.722694
-0.728113	-0.554667	4.101248	0.000199	0.723000
-0.842549	-0.464287	4.111245	0.000220	0.723138
-0.564284	-0.411809	4.121242	0.000167	0.723339
-0.681726	-0.256112	4.131238	0.000189	0.723604
-0.452524	-0.203366	4.141235	0.000146	0.723788
-0.373132	-0.114587	4.151232	0.000130	0.723991
-0.490552	0.046535	4.161229	0.000152	0.724266
0.000000	0.115239	4.171226	0.000060	0.724572

0.054952	0.756736	4.176230	0.000049	0.725846
-0.042376	2.049106	4.181235	0.000066	0.728334
0.309786	3.857517	4.186240	-0.000001	0.731968
0.972475	6.172605	4.191245	-0.000126	0.736668
1.637192	8.993660	4.196250	-0.000252	0.742305
2.224841	12.324146	4.201254	-0.000364	0.748839
2.873006	16.090590	4.206259	-0.000487	0.756154
3.564645	20.259863	4.211264	-0.000619	0.764161
4.114411	24.870480	4.216269	-0.000724	0.772849
4.944899	29.785220	4.221274	-0.000882	0.782082
6.070241	35.019586	4.226278	-0.001096	0.791874
7.394768	40.543141	4.231283	-0.001346	0.802118
8.699409	46.391698	4.236288	-0.001593	0.812794
9.874167	52.550555	4.241293	-0.001816	0.823826
10.810423	59.027204	4.246298	-0.001995	0.835179
11.595732	65.729923	4.251302	-0.002145	0.846714
12.518269	72.647639	4.256307	-0.002322	0.858488
13.034779	79.830583	4.261312	-0.002423	0.870418
13.894266	87.145942	4.266317	-0.002588	0.882495
14.363677	94.691368	4.271322	-0.002681	0.894666
14.960264	102.380749	4.276326	-0.002797	0.906932
15.483713	110.222579	4.281331	-0.002900	0.919250
15.942453	118.173547	4.286336	-0.002990	0.931554
16.635013	126.206750	4.291341	-0.003125	0.943882
17.086878	134.379760	4.296346	-0.003214	0.956195
17.579745	142.615171	4.301350	-0.003312	0.968454
18.153294	150.924914	4.306355	-0.003424	0.980686
18.851286	159.301139	4.311360	-0.003560	0.992894
19.548965	167.713118	4.316365	-0.003695	1.005003
19.904444	176.222760	4.321370	-0.003767	1.017021
20.469868	184.738535	4.326374	-0.003878	1.028956
20.986386	193.294534	4.331379	-0.003980	1.040798
21.147622	201.932824	4.336384	-0.004016	1.052535
21.646247	210.541190	4.341389	-0.004115	1.064179
22.046406	219.185910	4.346394	-0.004195	1.075723
23.353298	227.664411	4.351398	-0.004444	1.087131
24.118375	236.271394	4.356403	-0.004593	1.098465
24.697352	244.908294	4.361408	-0.004706	1.109681
25.184812	253.571288	4.366413	-0.004803	1.120797
25.371333	262.272227	4.371418	-0.004844	1.131786
25.779793	270.933773	4.376422	-0.004925	1.142668
26.163965	279.622357	4.381427	-0.005003	1.153475
26.514149	288.253477	4.386432	-0.005074	1.164105
27.391536	296.808529	4.391437	-0.005243	1.174655
27.626890	305.443395	4.396442	-0.005293	1.185075
27.867823	314.085171	4.401446	-0.005343	1.195413
28.458475	322.629166	4.406451	-0.005459	1.205618
28.960948	331.198209	4.411456	-0.005559	1.215749
29.310586	339.784276	4.416461	-0.005629	1.225785
29.520936	348.387396	4.421466	-0.005674	1.235732
30.014535	356.887825	4.426470	-0.005772	1.245537
30.773803	365.360919	4.431475	-0.005919	1.255285
31.319532	373.844730	4.436480	-0.006027	1.264930
31.816843	382.361658	4.441485	-0.006125	1.274528
33.967601	390.572316	4.446490	-0.006531	1.284025
34.533971	399.085275	4.451494	-0.006642	1.293489
35.132829	407.569833	4.456499	-0.006759	1.302860
35.732416	416.120841	4.461504	-0.006877	1.312235
35.904470	424.670127	4.466509	-0.006915	1.321465
36.185017	433.116397	4.471514	-0.006973	1.330541
37.257268	441.428894	4.476518	-0.007178	1.339553
38.372054	449.752173	4.481523	-0.007391	1.348523
38.760145	458.188296	4.486528	-0.007469	1.357425
39.123282	466.600380	4.491533	-0.007542	1.366240
39.691380	474.991994	4.496538	-0.007654	1.375012
40.042940	483.385271	4.501542	-0.007725	1.383693
40.812796	491.737292	4.506547	-0.007874	1.392348
41.046335	500.126324	4.511552	-0.007923	1.400897
41.682816	508.456526	4.516557	-0.008047	1.409402
42.138548	516.807649	4.521562	-0.008138	1.417847
42.434160	525.155610	4.526566	-0.008198	1.426212
43.198255	533.454458	4.531571	-0.008346	1.434556
43.649926	541.758549	4.536576	-0.008436	1.442806
44.208475	550.077301	4.541581	-0.008546	1.451040
44.524980	558.413194	4.546586	-0.008610	1.459206
44.982790	566.715050	4.551590	-0.008701	1.467316
45.283119	575.098136	4.556595	-0.008763	1.475434
45.648189	583.369329	4.561600	-0.008836	1.483411
46.214918	591.636671	4.566605	-0.008947	1.491372
46.280457	599.955382	4.571610	-0.008965	1.499263
46.624290	608.223674	4.576614	-0.009035	1.507107
47.228431	616.470428	4.581619	-0.009153	1.514930
47.656523	624.708415	4.586624	-0.009238	1.522678
48.642656	632.882555	4.591629	-0.009427	1.530412
49.097315	641.142571	4.596634	-0.009518	1.538105
49.542747	649.388827	4.601638	-0.009606	1.545746
50.150668	657.644703	4.606643	-0.009725	1.553383
50.385544	665.894829	4.611648	-0.009774	1.560921
50.805088	674.142212	4.616653	-0.009858	1.568448
50.952244	682.420061	4.621658	-0.009891	1.575927
51.605620	690.592007	4.626662	-0.010018	1.583348
52.248819	698.801423	4.631667	-0.010144	1.590767
52.553226	707.048421	4.636672	-0.010206	1.598136
52.798229	715.286098	4.641677	-0.010257	1.605454
53.192139	723.511690	4.646682	-0.010336	1.612749
53.528782	731.730277	4.651686	-0.010404	1.619998
54.072612	739.919422	4.656691	-0.010511	1.627217
54.211505	748.219844	4.661696	-0.010542	1.634444
54.912830	756.353827	4.666701	-0.010679	1.641573
55.194066	764.554780	4.671706	-0.010736	1.648671
55.783125	772.724003	4.676710	-0.010852	1.655754
56.184370	780.905963	4.681715	-0.010932	1.662791
56.607033	789.087640	4.686720	-0.011016	1.669801
57.306067	797.251131	4.691725	-0.011152	1.676804
57.743194	805.426430	4.696730	-0.011239	1.683752
58.145137	813.620325	4.701734	-0.011319	1.690683
58.496249	821.831079	4.706739	-0.011390	1.697592
58.676294	830.024335	4.711744	-0.011429	1.704436
59.410232	838.191202	4.716749	-0.011571	1.711303
59.856823	846.362842	4.721754	-0.011660	1.718109
59.990808	854.553392	4.726758	-0.011691	1.724864
60.531763	862.720163	4.731763	-0.011797	1.731624
60.948078	870.879765	4.736768	-0.011880	1.738337
61.300652	879.039407	4.741773	-0.011951	1.745015
61.723816	887.207302	4.746778	-0.012035	1.751684
62.239706	895.347518	4.751782	-0.012137	1.758316
62.427894	903.529278	4.756787	-0.012178	1.764916
62.795965	911.685149	4.761792	-0.012252	1.771492
63.197804	919.852554	4.766797	-0.012332	1.778058
63.271435	928.029962	4.771802	-0.012351	1.784567
63.539003	936.232509	4.776806	-0.012407	1.791095
64.002453	944.387151	4.781811	-0.012498	1.797586
64.344429	952.487122	4.786816	-0.012568	1.803996
64.651490	960.645014	4.791821	-0.012630	1.810425
64.808003	968.806395	4.796826	-0.012665	1.816815
65.152647	976.930285	4.801830	-0.012735	1.823175
65.428295	985.082839	4.806835	-0.012791	1.829528
65.587691	993.244048	4.811840	-0.012827	1.835852
66.195874	1001.333146	4.816845	-0.012945	1.842151
66.299386	1009.491269	4.821850	-0.012970	1.848422
66.714825	1017.624111	4.826854	-0.013053	1.854689
67.061277	1025.753364	4.831859	-0.013123	1.860924
67.233960	1033.890668	4.836864	-0.013161	1.867124
67.558812	1042.064824	4.841869	-0.013227	1.873349
67.781688	1050.180484	4.846874	-0.013274	1.879498
68.150325	1058.275597	4.851878	-0.013348	1.885627
68.602857	1066.402175	4.856883	-0.013438	1.891770
68.837583	1074.528817	4.861888	-0.013487	1.897868
69.135246	1082.656331	4.866893	-0.013548	1.903954
69.122645	1090.822801	4.871898	-0.013551	1.910015
69.344204	1098.959312	4.876902	-0.013598	1.916061
70.045928	1107.009147	4.881907	-0.013734	1.922077
70.427488	1115.109539	4.886912	-0.013810	1.928076
70.413786	1123.307866	4.891917	-0.013813	1.934084
70.844534	1131.387589	4.896922	-0.013899	1.940035
71.063452	1139.520702	4.901926	-0.013945	1.945985
71.505869	1147.664965	4.906931	-0.014033	1.951948
71.670184	1155.794170	4.911936	-0.014069	1.957852
71.832229	1163.898174	4.916941	-0.014105	1.963720
72.068459	1171.997243	4.921946	-0.014155	1.969574
72.188867	1180.137270	4.926950	-0.014182	1.975429
72.584525	1188.216394	4.931955	-0.014262	1.981251
72.855822	1196.305941	4.936960	-0.014318	1.987051
73.024649	1204.455707	4.941965	-0.014355	1.992866
73.237723	1212.550128	4.946970	-0.014400	1.998629
73.641833	1220.615242	4.951974	-0.014480	2.004375
74.000326	1228.711938	4.956979	-0.014553	2.010122
74.145736	1236.838071	4.961984	-0.014585	2.015851
74.788066	1244.884849	4.966989	-0.014710	2.021559
75.095396	1252.997850	4.971994	-0.014773	2.027263
75.286985	1261.146987	4.976998	-0.014814	2.032964
75.570132	1269.251067	4.982003	-0.014872	2.038627
75.808372	1277.322298	4.987008	-0.014922	2.044247
76.020255	1285.446498	4.992013	-0.014967	2.049886
76.266616	1293.558957	4.997018	-0.015019	2.055504
76.710664	1301.614885	5.002022	-0.015107	2.061088
77.263535	1309.687385	5.007027	-0.015215	2.066679
77.225422	1317.839199	5.012032	-0.015214	2.072250
77.561369	1325.941918	5.017037	-0.015282	2.077810
77.855813	1334.006942	5.022042	-0.015342	2.083325
78.331605	1342.086119	5.027046	-0.015436	2.088853
78.491417	1350.225795	5.032051	-0.015471	2.094376
79.115347	1358.258207	5.037056	-0.015593	2.099858
79.368631	1366.370643	5.042061	-0.015646	2.105343
79.535069	1374.503268	5.047066	-0.015682	2.110819
79.874976	1382.633047	5.052070	-0.015751	2.116295
80.292185	1390.683378	5.057075	-0.015834	2.121711
80.378317	1398.773191	5.062080	-0.015855	2.127109
80.798695	1406.861213	5.067085	-0.015939	2.132523
81.127745	1414.930650	5.072090	-0.016006	2.137902
81.410121	1423.000417	5.077094	-0.016064	2.143264
81.680380	1431.111317	5.082099	-0.016120	2.148638
82.160491	1439.185884	5.087104	-0.016215	2.153994
82.370417	1447.279732	5.092109	-0.016259	2.159324
82.452973	1455.362247	5.097114	-0.016280	2.164622
82.857312	1463.446103	5.102118	-0.016361	2.169938
83.116160	1471.555673	5.107123	-0.016415	2.175244
83.320876	1479.631599	5.112128	-0.016458	2.180510
83.583133	1487.727252	5.117133	-0.016512	2.185781
83.796546	1495.829512	5.122138	-0.016558	2.191040
84.309515	1503.900805	5.127142	-0.016659	2.196293
84.547357	1511.976994	5.132147	-0.016708	2.201511
84.665431	1520.050476	5.137152	-0.016736	2.206705
85.047309	1528.131057	5.142157	-0.016812	2.211915
85.387356	1536.206046	5.147162	-0.016881	2.217105
85.714997	1544.258808	5.152166	-0.016948	2.222267
85.981774	1552.343016	5.157171	-0.017003	2.227432
86.261524	1560.421962	5.162176	-0.017060	2.232583
86.660770	1568.507019	5.167181	-0.017140	2.237736
86.875165	1576.557151	5.172186	-0.017186	2.242839
87.191197	1584.640627	5.177190	-0.017250	2.247961
87.521047	1592.735879	5.182195	-0.017317	2.253079
87.898391	1600.787374	5.187200	-0.017393	2.258162
88.130292	1608.880737	5.192205	-0.017441	2.263248
88.222110	1616.972365	5.197210	-0.017464	2.268308
88.722549	1625.094281	5.202214	-0.017563	2.273412
89.217788	1633.133465	5.207219	-0.017660	2.278452
89.528964	1641.173144	5.212224	-0.017724	2.283465
89.648269	1649.265010	5.217229	-0.017751	2.288483
90.062436	1657.331091	5.222234	-0.017834	2.293499
90.392255	1665.382856	5.227238	-0.017901	2.298489
91.022602	1673.417698	5.232243	-0.018024	2.303482
91.460612	1681.462155	5.237248	-0.018111	2.308454
91.933814	1689.557232	5.242253	-0.018204	2.313449
92.246230	1697.622289	5.247258	-0.018268	2.318402
92.141299	1705.737955	5.252262	-0.018254	2.323340
92.611868	1713.790057	5.257267	-0.018347	2.328277
92.824551	1721.881817	5.262272	-0.018392	2.333205
93.205459	1729.940369	5.267277	-0.018468	2.338118
93.670286	1737.972946	5.272282	-0.018560	2.343010
93.926798	1746.063314	5.277286	-0.018614	2.347911
94.404260	1754.153588	5.282291	-0.018708	2.352819
94.914926	1762.188695	5.287296	-0.018808	2.357686
95.393168	1770.237577	5.292301	-0.018903	2.362549
95.603895	1778.321400	5.297306	-0.018948	2.367401
95.713079	1786.419657	5.302310	-0.018973	2.372244
96.171082	1794.484001	5.307315	-0.019064	2.377084
96.329829	1802.542167	5.312320	-0.019099	2.381887
96.556822	1810.634436	5.317325	-0.019147	2.386706
97.021450	1818.677120	5.322330	-0.019239	2.391504
97.382242	1826.730578	5.327334	-0.019312	2.396291
98.152025	1834.749807	5.332339	-0.019460	2.401081
98.540437	1842.790164	5.337344	-0.019538	2.405843
98.982301	1850.873397	5.342349	-0.019626	2.410625
99.195423	1858.982035	5.347354	-0.019671	2.415394
99.421740	1867.046606	5.352358	-0.019719	2.420130
99.783767	1875.117992	5.357363	-0.019792	2.424870
100.063029	1883.175336	5.362368	-0.019849	2.429587
100.548592	1891.329573	5.367373	-0.019945	2.434366
100.650942	1899.355773	5.372378	-0.019969	2.439033
100.909095	1907.386893	5.377382	-0.020023	2.443705
101.290608	1915.443019	5.382387	-0.020099	2.448392
101.418876	1923.519375	5.387392	-0.020129	2.453062
101.956854	1931.540979	5.392397	-0.020234	2.457723
102.473591	1939.576053	5.397402	-0.020336	2.462382
102.616117	1947.648617	5.402406	-0.020368	2.467024
102.872626	1955.745355	5.407411	-0.020421	2.471681
103.311467	1963.790326	5.412416	-0.020509	2.476312
103.581957	1971.846529	5.417421	-0.020564	2.480929
103.994213	1979.882224	5.422426	-0.020647	2.485536
104.144071	1987.950358	5.427430	-0.020680	2.490133
104.575793	1996.023175	5.432435	-0.020766	2.494745
104.835706	2004.066108	5.437440	-0.020820	2.499319
105.004453	2012.145391	5.442445	-0.020857	2.503899
105.544609	2020.177312	5.447450	-0.020963	2.508470
105.701478	2028.289373	5.452454	-0.020997	2.513050
106.056047	2036.343138	5.457459	-0.021069	2.517604
106.289434	2044.367680	5.462464	-0.021118	2.522124
106.648191	2052.422510	5.467469	-0.021190	2.526662
106.949494	2060.485152	5.472474	-0.021251	2.531191
107.293172	2068.544426	5.477478	-0.021321	2.535714
107.876787	2076.570050	5.482483	-0.021435	2.540227
108.243055	2084.608493	5.487488	-0.021509	2.544724
108.671323	2092.668988	5.492493	-0.021594	2.549229
108.924213	2100.768532	5.497498	-0.021646	2.553736
109.187033	2108.819440	5.502502	-0.021701	2.558208
109.563413	2116.846755	5.507507	-0.021776	2.562667
109.867967	2124.893683	5.512512	-0.021839	2.567124
110.398747	2132.950956	5.517517	-0.021943	2.571595
110.736257	2141.013367	5.522522	-0.022011	2.576048
111.100939	2149.059746	5.527526	-0.022084	2.580485
111.498899	2157.092913	5.532531	-0.022164	2.584911
111.659709	2165.164395	5.537536	-0.022199	2.589333
111.959209	2173.420286	5.542541	-0.022261	2.593857
112.343912	2181.412772	5.547546	-0.022338	2.598236
112.199192	2189.466937	5.552550	-0.022316	2.602606
112.453872	2197.489120	5.557555	-0.022369	2.606977
112.950356	2205.468616	5.562560	-0.022467	2.611335
113.258636	2213.529019	5.567565	-0.022530	2.615716
113.334761	2221.562774	5.572570	-0.022550	2.620060
113.445443	2229.599844	5.577574	-0.022576	2.624400
113.700744	2237.673054	5.582579	-0.022629	2.628763
113.924470	2245.729136	5.587584	-0.022676	2.633107
114.501423	2253.742038	5.592589	-0.022789	2.637444
114.477820	2261.799481	5.597594	-0.022790	2.641758
114.654709	2269.839037	5.602598	-0.022828	2.646068
114.988839	2277.894191	5.607603	-0.022896	2.650390
115.191812	2285.959119	5.612608	-0.022939	2.654702
115.705058	2293.980863	5.617613	-0.023040	2.659004
116.066129	2302.010955	5.622618	-0.023113	2.663293
116.461353	2310.051230	5.627622	-0.023192	2.667583
116.731116	2318.139425	5.632627	-0.023247	2.671883
116.799780	2326.212641	5.637632	-0.023266	2.676156
117.032890	2334.245125	5.642637	-0.023315	2.680410
117.423994	2342.242336	5.647642	-0.023393	2.684650
117.860644	2350.258203	5.652646	-0.023480	2.688895
118.158990	2358.364956	5.657651	-0.023541	2.693172
118.323971	2366.404933	5.662656	-0.023577	2.697400
118.977749	2374.410766	5.667661	-0.023704	2.701633
119.171190	2382.470483	5.672666	-0.023745	2.705859
119.438060	2390.539504	5.677670	-0.023801	2.710088
119.810233	2398.593700	5.682675	-0.023875	2.714309
119.816310	2406.647964	5.687680	-0.023882	2.718500
120.333197	2414.651325	5.692685	-0.023984	2.722691
120.792078	2422.704345	5.697690	-0.024074	2.726897
120.694748	2430.792780	5.702694	-0.024062	2.731080
120.835056	2438.879858	5.707699	-0.024093	2.735271
121.254879	2446.875506	5.712704	-0.024177	2.739426
121.635887	2454.912978	5.717709	-0.024253	2.743593
121.896816	2462.954019	5.722714	-0.024307	2.747748
122.324153	2471.029706	5.727718	-0.024392	2.751925
122.581421	2479.139766	5.732723	-0.024446	2.756103
122.938307	2487.107908	5.737728	-0.024518	2.760208
123.129180	2495.115541	5.742733	-0.024559	2.764317
123.292871	2503.183641	5.747738	-0.024595	2.768449
123.571702	2511.236956	5.752742	-0.024652	2.772574
123.811780	2519.299596	5.757747	-0.024702	2.776695
123.975721	2527.329794	5.762752	-0.024738	2.780789
124.512353	2535.316867	5.767757	-0.024843	2.784878
124.846978	2543.372723	5.772762	-0.024911	2.788983
125.108127	2551.444232	5.777766	-0.024965	2.793085
125.442525	2559.493949	5.782771	-0.025033	2.797175
125.652734	2567.531013	5.787776	-0.025078	2.801245
125.754520	2575.583727	5.792781	-0.025102	2.805311
126.023310	2583.601644	5.797786	-0.025158	2.809363
126.456119	2591.644750	5.802790	-0.025244	2.813431
126.558368	2599.714670	5.807795	-0.025268	2.817488
126.854171	2607.739197	5.812800	-0.025329	2.821527
127.329207	2615.749894	5.817805	-0.025423	2.825564
127.421103	2623.836085	5.822810	-0.025445	2.829611
127.449531	2631.930507	5.827814	-0.025456	2.833652
127.868236	2639.946320	5.832819	-0.025539	2.837671
128.135209	2647.963355	5.837824	-0.025594	2.841676
128.160919	2656.007279	5.842829	-0.025605	2.845675
128.403577	2664.036084	5.847834	-0.025655	2.849673
128.884887	2672.054368	5.852838	-0.025750	2.853673
129.444820	2680.075936	5.857843	-0.025860	2.857674
129.599738	2688.105377	5.862848	-0.025894	2.861651
130.230914	2696.120373	5.867853	-0.026017	2.865641
130.814251	2704.173188	5.872858	-0.026131	2.869641
130.999282	2712.255544	5.877862	-0.026171	2.873629
131.361127	2720.304023	5.882867	-0.026244	2.877604
131.411150	2728.343908	5.887872	-0.026259	2.881552
131.653624	2736.384238	5.892877	-0.026309	2.885505
131.932233	2744.418944	5.897882	-0.026367	2.889452
132.347431	2752.482226	5.902886	-0.026450	2.893416
132.506627	2760.550619	5.907891	-0.026485	2.897362
132.589010	2768.585403	5.912896	-0.026505	2.901282
132.815588	2776.612605	5.917901	-0.026553	2.905201
132.914040	2784.678409	5.922906	-0.026577	2.909127
132.953251	2792.798381	5.927910	-0.026590	2.913070
133.326974	2800.824940	5.932915	-0.026665	2.916981
134.019293	2808.766207	5.937920	-0.026799	2.920862
134.495262	2816.749868	5.942925	-0.026893	2.924746
134.485978	2824.833056	5.947930	-0.026897	2.928648
134.779425	2832.864826	5.952934	-0.026957	2.932536
134.970036	2840.932249	5.957939	-0.026998	2.936430
135.095234	2848.950037	5.962944	-0.027027	2.940292
135.675821	2856.927702	5.967949	-0.027140	2.944154
135.977942	2864.999751	5.972954	-0.027202	2.948041
136.116187	2873.047513	5.977958	-0.027233	2.951902
136.383675	2881.108269	5.982963	-0.027288	2.955772
136.616263	2889.102403	5.987968	-0.027337	2.959602
136.936724	2897.140792	5.992973	-0.027402	2.963454
137.133283	2905.178205	5.997978	-0.027444	2.967293
137.307432	2913.229855	6.002982	-0.027482	2.971133
137.490239	2921.307530	6.007987	-0.027522	2.974981
137.639393	2929.322347	6.012992	-0.027555	2.978792
138.028126	2937.334496	6.017997	-0.027633	2.982610
138.274659	2945.386773	6.023002	-0.027684	2.986434
138.504660	2953.424173	6.028006	-0.027732	2.990245
138.685204	2961.534763	6.033011	-0.027771	2.994084
139.018945	2969.506489	6.038016	-0.027839	2.997859
139.227559	2977.542793	6.043021	-0.027883	3.001654
139.501576	2985.560569	6.048026	-0.027940	3.005439
139.674003	2993.572695	6.053030	-0.027977	3.009212
139.992338	3001.668204	6.058035	-0.028042	3.013025
139.858689	3009.725532	6.063040	-0.028023	3.016794
140.169854	3017.754998	6.068045	-0.028086	3.020567
140.456219	3025.733100	6.073050	-0.028145	3.024310
140.580585	3033.767578	6.078054	-0.028173	3.028067
140.865250	3041.849697	6.083059	-0.028232	3.031849
141.135488	3049.873120	6.088064	-0.028287	3.035598
141.238291	3057.870905	6.093069	-0.028312	3.039323
141.477711	3065.908138	6.098074	-0.028362	3.043068
141.835247	3073.918961	6.103078	-0.028434	3.046801
142.096393	3081.998957	6.108083	-0.028488	3.050557
142.101092	3090.046592	6.113088	-0.028495	3.054282
142.437551	3098.076068	6.118093	-0.028563	3.058009
142.882534	3106.091540	6.123098	-0.028651	3.061731
142.838093	3114.140655	6.128102	-0.028648	3.065440
143.122601	3122.177442	6.133107	-0.028706	3.069155
143.618670	3130.256890	6.138112	-0.028804	3.072894
143.805774	3138.315995	6.143117	-0.028845	3.076605
143.929062	3146.302908	6.148122	-0.028873	3.080276
144.000546	3154.288990	6.153126	-0.028892	3.083939
144.437602	3162.334989	6.158131	-0.028979	3.087643
144.380735	3170.382663	6.163136	-0.028973	3.091319
144.657270	3178.437089	6.168141	-0.029030	3.095010
144.876101	3186.450918	6.173146	-0.029077	3.098675
145.100698	3194.445662	6.178150	-0.029124	3.102328
145.279122	3202.510870	6.183155	-0.029162	3.106006
145.341835	3210.555377	6.188160	-0.029180	3.109665
145.666062	3218.625281	6.193165	-0.029245	3.113343
146.204060	3226.611270	6.198170	-0.029351	3.116988
146.292735	3234.626025	6.203174	-0.029373	3.120622
146.648146	3242.645123	6.208179	-0.029445	3.124265
146.468810	3250.701820	6.213184	-0.029417	3.127897
146.949821	3258.726778	6.218189	-0.029512	3.131540
147.170697	3266.800153	6.223194	-0.029558	3.135189
147.384702	3274.789368	6.228198	-0.029604	3.138796
147.594033	3282.841833	6.233203	-0.029648	3.142426
147.716826	3290.857962	6.238208	-0.029676	3.146033
148.007262	3298.881578	6.243213	-0.029736	3.149645
148.145940	3306.973989	6.248218	-0.029767	3.153278
148.338451	3314.977750	6.253222	-0.029808	3.156870
148.864127	3322.981384	6.258227	-0.029912	3.160471
148.916752	3330.996266	6.263232	-0.029927	3.164053
148.960707	3339.059616	6.268237	-0.029941	3.167652
149.117067	3347.114992	6.273242	-0.029975	3.171248
149.275216	3355.145736	6.278246	-0.030010	3.174829
149.536329	3363.182749	6.283251	-0.030064	3.178414
149.729774	3371.174276	6.288256	-0.030106	3.181971
150.132030	3379.218910	6.293261	-0.030186	3.185557
150.338288	3387.247156	6.298266	-0.030230	3.189123
150.530975	3395.282970	6.303270	-0.030271	3.192687
150.650914	3403.351053	6.308275	-0.030299	3.196259
150.751419	3411.320433	6.313280	-0.030323	3.199783
151.169556	3419.341447	6.318285	-0.030406	3.203338
151.508328	3427.387614	6.323290	-0.030475	3.206898
151.483961	3435.431085	6.328294	-0.030476	3.210437
151.533974	3443.526150	6.333299	-0.030491	3.213998
151.771794	3451.522919	6.338304	-0.030540	3.217519
152.048978	3459.537694	6.343309	-0.030597	3.221047
152.194693	3467.554475	6.348314	-0.030630	3.224565
152.312217	3475.582729	6.353318	-0.030657	3.228084
152.728636	3483.664066	6.358323	-0.030740	3.231635
152.872632	3491.737681	6.363328	-0.030772	3.235167
153.087530	3499.692599	6.368333	-0.030818	3.238646
153.226516	3507.730605	6.373338	-0.030849	3.242154
153.381619	3515.718494	6.378342	-0.030883	3.245638
153.765644	3523.736284	6.383347	-0.030960	3.249140
153.681795	3531.816837	6.388352	-0.030950	3.252646
153.873854	3539.874936	6.393357	-0.030991	3.256150
154.114131	3547.858117	6.398362	-0.031042	3.259620
154.298476	3555.855772	6.403366	-0.031081	3.263090
154.659784	3563.907975	6.408371	-0.031154	3.266587
154.777526	3571.937703	6.413376	-0.031181	3.270061
155.154995	3579.990756	6.418381	-0.031257	3.273552
155.284930	3588.028705	6.423386	-0.031287	3.277022
155.667034	3596.007423	6.428390	-0.031363	3.280473
155.870586	3604.060256	6.433395	-0.031407	3.283945
155.978487	3612.094733	6.438400	-0.031432	3.287402
156.254301	3620.156807	6.443405	-0.031489	3.290874
156.463423	3628.175256	6.448410	-0.031534	3.294321
156.307906	3636.204276	6.453414	-0.031510	3.297754
156.531946	3644.249248	6.458419	-0.031557	3.301206
156.740160	3652.242790	6.463424	-0.031601	3.304631
157.070291	3660.265327	6.468429	-0.031668	3.308069
157.284483	3668.343292	6.473434	-0.031714	3.311524
157.430996	3676.356642	6.478438	-0.031746	3.314944
157.607830	3684.396942	6.483443	-0.031785	3.318374
158.069640	3692.376423	6.488448	-0.031876	3.321784
158.116471	3700.389125	6.493453	-0.031890	3.325190
158.331626	3708.427663	6.498458	-0.031936	3.328610
158.153892	3716.494299	6.503462	-0.031908	3.332023
158.619056	3724.533522	6.508467	-0.032000	3.335445
158.793170	3732.512879	6.513472	-0.032038	3.338827
159.091823	3740.524304	6.518477	-0.032099	3.342224
159.344707	3748.565764	6.523482	-0.032152	3.345629
159.462428	3756.586535	6.528486	-0.032179	3.349016
159.859158	3764.649170	6.533491	-0.032258	3.352428
159.905588	3772.694062	6.538496	-0.032272	3.355816
160.341868	3780.669703	6.543501	-0.032359	3.359186
160.485805	3788.703976	6.548506	-0.032391	3.362566
160.610295	3796.733190	6.553510	-0.032420	3.365940
160.738034	3804.758327	6.558515	-0.032449	3.369309
160.850903	3812.836839	6.563520	-0.032476	3.372696
161.289003	3820.868957	6.568525	-0.032563	3.376072
161.265921	3828.874533	6.573530	-0.032564	3.379417
161.359705	3836.878131	6.578534	-0.032587	3.382763
161.613249	3844.951820	6.583539	-0.032639	3.386139
161.776404	3852.970864	6.588544	-0.032675	3.389487
162.174779	3861.046395	6.593549	-0.032755	3.392863
162.383929	3869.101748	6.598554	-0.032799	3.396220
162.458424	3877.035874	6.603558	-0.032818	3.399519
162.864481	3885.046352	6.608563	-0.032900	3.402858
163.077419	3893.052381	6.613568	-0.032945	3.406185
163.217479	3901.075427	6.618573	-0.032976	3.409514
163.539104	3909.132825	6.623578	-0.033041	3.412859
163.944496	3917.134685	6.628582	-0.033122	3.416181
163.975268	3925.173221	6.633587	-0.033134	3.419502
164.029228	3933.169992	6.638592	-0.033149	3.422804
164.341715	3941.225995	6.643597	-0.033213	3.426135
164.601731	3949.228312	6.648602	-0.033267	3.429440
164.643971	3957.287431	6.653606	-0.033280	3.432757
164.812385	3965.364587	6.658611	-0.033317	3.436082
165.000845	3973.339244	6.663616	-0.033357	3.439363
165.087908	3981.361832	6.668621	-0.033379	3.442657
165.418488	3989.383077	6.673626	-0.033446	3.445956
165.447907	3997.385416	6.678630	-0.033457	3.449233
165.974770	4005.457572	6.683635	-0.033560	3.452553
166.115234	4013.533694	6.688640	-0.033592	3.455857
166.289280	4021.494806	6.693645	-0.033630	3.459113
166.564237	4029.551149	6.698650	-0.033686	3.462408
166.607410	4037.557170	6.703654	-0.033700	3.465672
166.934510	4045.603375	6.708659	-0.033766	3.468958
167.132408	4053.643837	6.713664	-0.033808	3.472235
167.210870	4061.694548	6.718669	-0.033829	3.475509
167.581736	4069.688206	6.723674	-0.033903	3.478765
167.679014	4077.684944	6.728678	-0.033927	3.482012
167.659898	4085.721489	6.733683	-0.033928	3.485267
167.854013	4093.734909	6.738688	-0.033970	3.488517
168.123993	4101.764630	6.743693	-0.034026	3.491773
168.407120	4109.803269	6.748698	-0.034084	3.495030
168.443497	4117.816165	6.753702	-0.034096	3.498266
168.968870	4125.842623	6.758707	-0.034199	3.501519
169.101474	4133.810360	6.763712	-0.034229	3.504734
169.359098	4141.882112	6.768717	-0.034283	3.507991
169.451423	4149.943183	6.773722	-0.034306	3.511236
169.633344	4157.941117	6.778726	-0.034345	3.514455
170.040713	4165.965734	6.783731	-0.034426	3.517688
170.147341	4173.989812	6.788736	-0.034451	3.520910
170.155479	4181.964118	6.793741	-0.034458	3.524105
170.363143	4190.028779	6.798746	-0.034502	3.527340
170.577144	4198.067663	6.803750	-0.034548	3.530561
170.840693	4206.142289	6.808755	-0.034602	3.533796
171.059162	4214.113618	6.813760	-0.034648	3.536985
171.074328	4222.149871	6.818765	-0.034657	3.540190
171.207945	4230.168835	6.823770	-0.034687	3.543390
171.490713	4238.205105	6.828774	-0.034745	3.546598
171.806115	4246.247916	6.833779	-0.034809	3.549806
172.083724	4254.377219	6.838784	-0.034866	3.553045
172.237921	4262.395816	6.843789	-0.034901	3.556233
172.333168	4270.340237	6.848794	-0.034924	3.559387
172.379102	4278.328509	6.853798	-0.034938	3.562554
172.778526	4286.347500	6.858803	-0.035018	3.565741
173.155857	4294.354165	6.863808	-0.035093	3.568920
173.343617	4302.382867	6.868813	-0.035134	3.572099
173.611326	4310.447757	6.873818	-0.035189	3.575291
173.620172	4318.414616	6.878822	-0.035196	3.578435
173.814123	4326.474834	6.883827	-0.035238	3.581618
173.952522	4334.497187	6.888832	-0.035269	3.584781
173.984959	4342.508980	6.893837	-0.035280	3.587935
174.277684	4350.559866	6.898842	-0.035340	3.591108
174.432393	4358.555608	6.903846	-0.035374	3.594253
174.519032	4366.594366	6.908851	-0.035396	3.597411
174.699339	4374.596871	6.913856	-0.035435	3.600554
174.800066	4382.600192	6.918861	-0.035459	3.603692
174.905363	4390.641336	6.923866	-0.035484	3.606842
175.154183	4398.631435	6.928870	-0.035536	3.609974
175.555418	4406.694516	6.933875	-0.035616	3.613136
175.580468	4414.754664	6.938880	-0.035626	3.616283
175.707763	4422.738565	6.943885	-0.035655	3.619400
175.972839	4430.762196	6.948890	-0.035710	3.622535
176.410910	4438.761512	6.953894	-0.035797	3.625661
176.528234	4446.816877	6.958899	-0.035825	3.628798
176.576955	4454.880847	6.963904	-0.035839	3.631934
176.933957	4462.920711	6.968909	-0.035911	3.635066
177.226451	4470.910173	6.973914	-0.035971	3.638174
177.048192	4478.958515	6.978918	-0.035943	3.641289
177.317274	4486.919110	6.983923	-0.035999	3.644380
177.493155	4494.951109	6.988928	-0.036037	3.647494
177.746326	4502.966984	6.993933	-0.036089	3.650600
178.124706	4511.051572	6.998938	-0.036165	3.653733
178.301916	4519.063147	7.003942	-0.036204	3.656831
178.293507	4527.090989	7.008947	-0.036208	3.659927
178.672445	4535.079905	7.013952	-0.036284	3.663015
178.835098	4543.107405	7.018957	-0.036319	3.666111
178.981010	4551.138839	7.023962	-0.036352	3.669204
178.914292	4559.186548	7.028966	-0.036345	3.672296
179.404424	4567.206930	7.033971	-0.036442	3.675389
179.659015	4575.206090	7.038976	-0.036494	3.678465
179.587172	4583.232200	7.043981	-0.036487	3.681541
179.812569	4591.219149	7.048986	-0.036534	3.684606
179.939050	4599.252052	7.053990	-0.036563	3.687684
179.934994	4607.315873	7.058995	-0.036568	3.690768
180.092303	4615.373361	7.064000	-0.036602	3.693851
180.315799	4623.345781	7.069005	-0.036649	3.696900
180.635551	4631.369345	7.074010	-0.036714	3.699969
180.573679	4639.364826	7.079014	-0.036708	3.703016
180.816065	4647.419227	7.084019	-0.036759	3.706089
181.025258	4655.428414	7.089024	-0.036803	3.709142
181.027261	4663.524246	7.094029	-0.036809	3.712220
181.375703	4671.599521	7.099034	-0.036879	3.715297
181.464170	4679.538751	7.104038	-0.036901	3.718313
181.745369	4687.551988	7.109043	-0.036959	3.721359
181.860310	4695.517446	7.114048	-0.036986	3.724380
182.011110	4703.525910	7.119053	-0.037019	3.727416
182.307003	4711.569731	7.124058	-0.037080	3.730467
182.251466	4719.592969	7.129062	-0.037075	3.733499
182.530903	4727.652819	7.134067	-0.037133	3.736550
182.859748	4735.638488	7.139072	-0.037199	3.739572
182.854791	4743.649237	7.144077	-0.037204	3.742593
183.002925	4751.700815	7.149082	-0.037237	3.745630
183.413509	4759.675434	7.154086	-0.037319	3.748642
183.548959	4767.769243	7.159091	-0.037349	3.751690
183.792355	4775.793213	7.164096	-0.037400	3.754712
184.105953	4783.786159	7.169101	-0.037464	3.757721
184.416211	4791.839128	7.174106	-0.037527	3.760750
184.497483	4799.802016	7.179110	-0.037548	3.763738
184.642329	4807.857411	7.184115	-0.037580	3.766760
184.938072	4815.854242	7.189120	-0.037641	3.769760
185.053134	4823.901133	7.194125	-0.037667	3.772773
185.264144	4831.975437	7.199130	-0.037712	3.775796
185.571444	4839.930067	7.204134	-0.037775	3.778773
185.833309	4847.999306	7.209139	-0.037829	3.781791
185.881114	4855.999177	7.214144	-0.037843	3.784775
186.111255	4864.000344	7.219149	-0.037892	3.787761
186.297070	4872.068466	7.224154	-0.037932	3.790768
186.616404	4880.095684	7.229158	-0.037997	3.793762
186.865067	4888.145340	7.234163	-0.038048	3.796759
187.118718	4896.095219	7.239168	-0.038101	3.799717
187.217941	4904.112681	7.244173	-0.038125	3.802695
187.153203	4912.148627	7.249178	-0.038118	3.805673
187.477926	4920.121707	7.254182	-0.038184	3.808634
187.813152	4928.204293	7.259187	-0.038252	3.811634
187.811727	4936.227686	7.264192	-0.038257	3.814602
188.100594	4944.209264	7.269197	-0.038316	3.817558
188.394961	4952.221366	7.274202	-0.038377	3.820524
188.497326	4960.224639	7.279206	-0.038401	3.823480
188.527561	4968.304350	7.284211	-0.038412	3.826460
188.709778	4976.285075	7.289216	-0.038452	3.829405
188.579710	4984.374632	7.294221	-0.038433	3.832381
188.810295	4992.383752	7.299226	-0.038481	3.835332
188.836205	5000.355502	7.304230	-0.038491	3.838263
189.180103	5008.381761	7.309235	-0.038561	3.841219
189.365564	5016.363696	7.314240	-0.038601	3.844153
189.423856	5024.410022	7.319245	-0.038617	3.847105
189.893029	5032.419199	7.324250	-0.038710	3.850050
190.128114	5040.448579	7.329254	-0.038759	3.852996
190.388818	5048.493890	7.334259	-0.038813	3.855945
190.653638	5056.538420	7.339264	-0.038868	3.858892
190.889609	5064.539520	7.344269	-0.038917	3.861820
191.249456	5072.567390	7.349274	-0.038990	3.864758
191.311380	5080.560436	7.354278	-0.039007	3.867675
191.650761	5088.612142	7.359283	-0.039075	3.870617
191.605893	5096.891594	7.364288	-0.039073	3.873632
191.807299	5104.857845	7.369293	-0.039116	3.876535
191.992025	5112.769232	7.374298	-0.039155	3.879416
192.118221	5120.730113	7.379302	-0.039184	3.882312
192.343277	5128.765681	7.384307	-0.039232	3.885235
192.442758	5136.758143	7.389312	-0.039255	3.888137
192.548082	5144.758040	7.394317	-0.039280	3.891040
192.671657	5152.838852	7.399322	-0.039309	3.893970
192.805825	5160.820015	7.404326	-0.039339	3.896862
193.089419	5168.822643	7.409331	-0.039398	3.899763
193.129929	5176.870842	7.414336	-0.039411	3.902673
193.283130	5184.825835	7.419341	-0.039445	3.905550
193.406048	5192.877451	7.424346	-0.039473	3.908459
193.581845	5200.907285	7.429350	-0.039511	3.911358
193.762008	5208.961998	7.434355	-0.039550	3.914265
193.881507	5216.979935	7.439360	-0.039578	3.917155
194.069932	5224.916157	7.444365	-0.039618	3.920015
194.186587	5232.986966	7.449370	-0.039645	3.922919
194.297099	5240.990255	7.454374	-0.039671	3.925798
194.457206	5249.023059	7.459379	-0.039707	3.928685
194.765400	5257.051788	7.464384	-0.039769	3.931572
194.782095	5265.051518	7.469389	-0.039778	3.934441
195.138439	5273.081113	7.474394	-0.039850	3.937324
195.277077	5281.072626	7.479398	-0.039881	3.940188
195.435692	5289.101328	7.484403	-0.039916	3.943063
195.768382	5297.133492	7.489408	-0.039983	3.945941
196.009456	5305.121097	7.494413	-0.040034	3.948799
196.187791	5313.204278	7.499418	-0.040072	3.951687
196.340072	5321.212432	7.504422	-0.040106	3.954547
196.491126	5329.260683	7.509427	-0.040140	3.957418
196.857513	5337.205364	7.514432	-0.040213	3.960255
197.016836	5345.200095	7.519437	-0.040248	3.963103
197.342225	5353.252393	7.524442	-0.040314	3.965973
197.270918	5361.230331	7.529446	-0.040307	3.968808
197.453583	5369.288917	7.534451	-0.040346	3.971673
197.717537	5377.348676	7.539456	-0.040401	3.974538
197.589704	5385.368577	7.544461	-0.040382	3.977380
197.870215	5393.368809	7.549466	-0.040440	3.980220
197.698802	5401.399560	7.554470	-0.040414	3.983062
198.253549	5409.417137	7.559475	-0.040522	3.985908
198.513051	5417.431431	7.564480	-0.040576	3.988747
198.260400	5425.469036	7.569485	-0.040534	3.991583
198.545646	5433.515802	7.574490	-0.040593	3.994430
198.858184	5441.527361	7.579494	-0.040657	3.997262
199.020718	5449.548044	7.584499	-0.040692	4.000093
198.977217	5457.549283	7.589504	-0.040690	4.002912
199.236915	5465.563718	7.594509	-0.040743	4.005738
199.440119	5473.574051	7.599514	-0.040787	4.008560
199.450243	5481.602335	7.604518	-0.040794	4.011383
199.529588	5489.636750	7.609523	-0.040814	4.014208
199.858567	5497.692447	7.614528	-0.040881	4.017042
199.859938	5505.661678	7.619533	-0.040887	4.019838
200.171622	5513.703839	7.624538	-0.040950	4.022663
200.197531	5521.698376	7.629542	-0.040960	4.025464
200.591112	5529.743981	7.634547	-0.041039	4.028288
200.835513	5537.784041	7.639552	-0.041090	4.031105
200.813746	5545.874408	7.644557	-0.041091	4.033933
201.000740	5553.886374	7.649562	-0.041132	4.036735
201.110450	5561.808026	7.654566	-0.041158	4.039503
201.288405	5569.835181	7.659571	-0.041196	4.042307
201.448545	5577.824860	7.664576	-0.041231	4.045095
201.551579	5585.812683	7.669581	-0.041256	4.047880
201.785215	5593.889351	7.674586	-0.041305	4.050695
201.987461	5601.907541	7.679590	-0.041348	4.053488
202.360353	5609.935905	7.684595	-0.041423	4.056285
202.549589	5617.920981	7.689600	-0.041464	4.059063
202.596489	5625.936386	7.694605	-0.041478	4.061847
202.803121	5633.936343	7.699610	-0.041522	4.064626
202.807271	5641.957367	7.704614	-0.041528	4.067407
203.077358	5650.009101	7.709619	-0.041584	4.070201
203.087124	5658.079756	7.714624	-0.041591	4.072996
202.985873	5666.034999	7.719629	-0.041577	4.075747
203.398698	5674.039046	7.724634	-0.041660	4.078521
203.582800	5682.068714	7.729638	-0.041699	4.081298
203.765817	5690.064186	7.734643	-0.041739	4.084062
203.837347	5698.108487	7.739648	-0.041758	4.086839
203.936277	5706.101070	7.744653	-0.041781	4.089596
204.350980	5714.197275	7.749658	-0.041864	4.092392
204.209427	5722.177618	7.754662	-0.041843	4.095138
204.380164	5730.238259	7.759667	-0.041881	4.097915
204.726685	5738.181421	7.764672	-0.041950	4.100651
204.756451	5746.166749	7.769677	-0.041961	4.103396
204.861245	5754.265510	7.774682	-0.041986	4.106179
204.985048	5762.262632	7.779686	-0.042015	4.108926
205.223256	5770.335498	7.784691	-0.042065	4.111698
205.494603	5778.378958	7.789696	-0.042121	4.114458
205.489808	5786.343461	7.794701	-0.042125	4.117186
205.579788	5794.340740	7.799706	-0.042147	4.119925
205.547092	5802.372585	7.804710	-0.042147	4.122672
205.927949	5810.370776	7.809715	-0.042223	4.125411
205.825620	5818.409542	7.814720	-0.042209	4.128156
206.136861	5826.394623	7.819725	-0.042273	4.130885
206.404293	5834.486494	7.824730	-0.042328	4.133649
206.590453	5842.459503	7.829734	-0.042368	4.136370
206.694628	5850.495788	7.834739	-0.042393	4.139109
207.004476	5858.534690	7.839744	-0.042456	4.141850
207.008417	5866.480689	7.844749	-0.042462	4.144554
207.279979	5874.567554	7.849754	-0.042518	4.147306
207.274787	5882.563017	7.854758	-0.042523	4.150023
207.327551	5890.609526	7.859763	-0.042538	4.152756
207.773300	5898.667962	7.864768	-0.042626	4.155496
207.928939	5906.603790	7.869773	-0.042661	4.158189
208.183529	5914.652019	7.874778	-0.042714	4.160920
208.272272	5922.613565	7.879782	-0.042736	4.163617
208.488980	5930.691314	7.884787	-0.042781	4.166354
208.489593	5938.705130	7.889792	-0.042787	4.169064
208.646848	5946.717986	7.894797	-0.042822	4.171774
209.144386	5954.725695	7.899802	-0.042920	4.174485
209.067789	5962.740290	7.904806	-0.042911	4.177189
209.224786	5970.774570	7.909811	-0.042946	4.179901
209.549977	5978.793804	7.914816	-0.043012	4.182609
209.620561	5986.741392	7.919821	-0.043030	4.185287
209.686716	5994.816690	7.924826	-0.043048	4.188006
209.941409	6002.820658	7.929830	-0.043101	4.190702
210.170132	6010.923603	7.934835	-0.043149	4.193429
210.321306	6018.982346	7.939840	-0.043182	4.196139
210.272052	6026.872287	7.944845	-0.043179	4.198788
210.289881	6034.959581	7.949850	-0.043187	4.201502
210.518858	6042.848115	7.954854	-0.043235	4.204150
210.824752	6050.908918	7.959859	-0.043298	4.206855
211.004085	6058.938854	7.964864	-0.043337	4.209547
210.957042	6066.952959	7.969869	-0.043333	4.212229
211.078847	6075.019299	7.974874	-0.043362	4.214928
211.242778	6082.981229	7.979878	-0.043397	4.217592
211.476416	6090.960191	7.984883	-0.043446	4.220260
211.623379	6099.024531	7.989888	-0.043479	4.222954
211.586065	6107.005960	7.994893	-0.043478	4.225617
211.837016	6115.098179	7.999898	-0.043530	4.228317
211.823316	6123.069418	8.004902	-0.043533	4.230974
211.929045	6131.140658	8.009907	-0.043558	4.233663
212.242791	6139.158522	8.014912	-0.043622	4.236334
212.301098	6147.110982	8.019917	-0.043638	4.238980
212.723604	6155.178320	8.024922	-0.043722	4.241665
212.614239	6163.101485	8.029926	-0.043707	4.244296
213.094024	6171.173827	8.034931	-0.043802	4.246980
213.269517	6179.200674	8.039936	-0.043840	4.249645
213.219081	6187.233251	8.044941	-0.043836	4.252308
213.578431	6195.223751	8.049946	-0.043908	4.254959
213.710648	6203.279356	8.054950	-0.043938	4.257627
213.718393	6211.276451	8.059955	-0.043945	4.260274
213.903950	6219.324731	8.064960	-0.043985	4.262937
214.034218	6227.293621	8.069965	-0.044015	4.265572
214.392354	6235.398543	8.074970	-0.044087	4.268253
214.442311	6243.371141	8.079974	-0.044102	4.270885
214.806937	6251.448372	8.084979	-0.044175	4.273552
215.072638	6259.503063	8.089984	-0.044230	4.276210
215.047200	6267.414936	8.094989	-0.044231	4.278817
215.183015	6275.483050	8.099994	-0.044262	4.281475
215.378104	6283.427565	8.104998	-0.044303	4.284090
215.527097	6291.488339	8.110003	-0.044337	4.286743
215.695729	6299.484318	8.115008	-0.044373	4.289372
215.808997	6307.527536	8.120013	-0.044400	4.292015
215.903396	6315.564813	8.125018	-0.044423	4.294654
216.053324	6323.567645	8.130022	-0.044456	4.297280
216.270590	6331.538566	8.135027	-0.044502	4.299895
216.531252	6339.573440	8.140032	-0.044556	4.302530
216.331503	6347.593807	8.145037	-0.044524	4.305155
216.736452	6355.632375	8.150042	-0.044605	4.307788
216.741630	6363.636707	8.155046	-0.044612	4.310406
216.905154	6371.677587	8.160051	-0.044647	4.313036
217.229544	6379.715914	8.165056	-0.044713	4.315664
217.468275	6387.669398	8.170061	-0.044763	4.318262
217.265213	6395.722985	8.175066	-0.044731	4.320888
217.211316	6403.704292	8.180070	-0.044726	4.323490
217.738913	6411.709066	8.185075	-0.044830	4.326102
217.901830	6419.721198	8.190080	-0.044866	4.328712
217.940662	6427.773582	8.195085	-0.044878	4.331333
218.047848	6435.817861	8.200090	-0.044904	4.333950
218.158492	6443.846805	8.205094	-0.044930	4.336561
218.544109	6451.802682	8.210099	-0.045007	4.339148
218.745524	6459.863549	8.215104	-0.045050	4.341766
218.800960	6467.767837	8.220109	-0.045066	4.344331
218.974440	6475.913222	8.225114	-0.045103	4.346974
219.089034	6483.869228	8.230118	-0.045130	4.349553
219.227325	6491.933664	8.235123	-0.045161	4.352166
219.295007	6500.051709	8.240128	-0.045179	4.354794
219.274159	6508.014271	8.245133	-0.045181	4.357370
219.657856	6515.957134	8.250138	-0.045258	4.359940
219.872299	6523.941016	8.255142	-0.045303	4.362521
219.811876	6531.937943	8.260147	-0.045297	4.365103
219.896361	6540.008421	8.265152	-0.045319	4.367708
220.071661	6547.970685	8.270157	-0.045357	4.370277
220.144032	6556.028778	8.275162	-0.045376	4.372875
220.233518	6564.047758	8.280166	-0.045398	4.375458
220.402593	6572.089459	8.285171	-0.045435	4.378048
220.609006	6580.077083	8.290176	-0.045478	4.380620
220.777087	6588.028420	8.295181	-0.045515	4.383178
220.907211	6596.091072	8.300186	-0.045545	4.385769
221.132431	6604.147156	8.305190	-0.045592	4.388358
221.134818	6612.125387	8.310195	-0.045598	4.390919
221.249303	6620.194941	8.315200	-0.045625	4.393509
221.574581	6628.226759	8.320205	-0.045691	4.396085
221.952250	6636.200171	8.325210	-0.045767	4.398642
221.822945	6644.228746	8.330214	-0.045748	4.401213
222.070720	6652.203081	8.335219	-0.045799	4.403766
222.277258	6660.259952	8.340224	-0.045843	4.406344
222.259872	6668.236326	8.345229	-0.045846	4.408894
222.727390	6676.287830	8.350234	-0.045938	4.411469
222.788180	6684.324194	8.355238	-0.045955	4.414035
222.795803	6692.370982	8.360243	-0.045962	4.416603
222.564623	6700.374213	8.365248	-0.045924	4.419154
222.912632	6708.393829	8.370253	-0.045994	4.421712
223.151208	6716.368885	8.375258	-0.046044	4.424254
223.019430	6724.408020	8.380262	-0.046025	4.426813
223.308753	6732.405418	8.385267	-0.046084	4.429359
223.647163	6740.457906	8.390272	-0.046153	4.431921
223.941590	6748.508939	8.395277	-0.046213	4.434481
223.822033	6756.559691	8.400282	-0.046196	4.437037
223.950565	6764.500480	8.405286	-0.046226	4.439559
224.145982	6772.486280	8.410291	-0.046267	4.442093
224.597678	6780.499903	8.415296	-0.046357	4.444636
224.305047	6788.530046	8.420301	-0.046308	4.447180
224.502583	6796.546505	8.425306	-0.046350	4.449719
224.568128	6804.593978	8.430310	-0.046368	4.452267
224.654677	6812.568832	8.435315	-0.046389	4.454790
225.011862	6820.638741	8.440320	-0.046461	4.457343
225.128918	6828.594784	8.445325	-0.046488	4.459857
225.100851	6836.658960	8.450330	-0.046489	4.462404
225.318485	6844.636790	8.455334	-0.046535	4.464923
225.818545	6852.687230	8.460339	-0.046633	4.467464
225.479086	6860.713379	8.465344	-0.046575	4.469993
225.474072	6868.710475	8.470349	-0.046580	4.472513
225.960800	6876.745359	8.475354	-0.046676	4.475045
226.037065	6884.738819	8.480358	-0.046696	4.477561
225.971960	6892.741291	8.485363	-0.046689	4.480078
226.320727	6900.783673	8.490368	-0.046759	4.482607
226.517234	6908.734893	8.495373	-0.046801	4.485106
226.704788	6916.781222	8.500378	-0.046842	4.487634
226.680422	6924.798427	8.505382	-0.046843	4.490150
226.977633	6932.839932	8.510387	-0.046903	4.492673
227.158026	6940.904121	8.515392	-0.046942	4.495201
227.102078	6948.887397	8.520397	-0.046937	4.497702
227.232377	6956.892368	8.525402	-0.046967	4.500209
227.390821	6964.857707	8.530406	-0.047002	4.502703
227.522035	6972.870698	8.535411	-0.047032	4.505209
227.662864	6980.936083	8.540416	-0.047064	4.507731
227.762209	6988.862455	8.545421	-0.047087	4.510207
227.907636	6997.013883	8.550426	-0.047120	4.512753
228.085814	7005.044637	8.555430	-0.047159	4.515260
228.243546	7013.011003	8.560435	-0.047193	4.517745
228.467814	7020.987339	8.565440	-0.047241	4.520232
228.490180	7028.983668	8.570445	-0.047250	4.522723
228.671453	7036.983296	8.575450	-0.047289	4.525215
228.688637	7045.030689	8.580455	-0.047298	4.527719
228.581155	7053.007084	8.585459	-0.047283	4.530200
228.897950	7061.089528	8.590464	-0.047348	4.532713
229.153532	7069.056363	8.595469	-0.047401	4.535189
229.146996	7077.174083	8.600474	-0.047405	4.537710
228.946770	7085.128422	8.605479	-0.047373	4.540178
229.233890	7093.089258	8.610483	-0.047432	4.542648
229.520128	7101.137153	8.615488	-0.047491	4.545143
229.513127	7109.110528	8.620493	-0.047495	4.547613
229.543595	7117.142508	8.625498	-0.047506	4.550101
229.674418	7125.199593	8.630503	-0.047536	4.552595
229.767250	7133.228022	8.635507	-0.047559	4.555078
229.937953	7141.246380	8.640512	-0.047596	4.557557
230.099548	7149.231824	8.645517	-0.047631	4.560025
230.170256	7157.256425	8.650522	-0.047650	4.562503
230.103080	7165.251575	8.655527	-0.047643	4.564971
230.458318	7173.293974	8.660531	-0.047714	4.567452
230.724435	7181.304750	8.665536	-0.047769	4.569922
230.617880	7189.345563	8.670541	-0.047755	4.572400
230.736168	7197.361591	8.675546	-0.047783	4.574869
230.951476	7205.382726	8.680551	-0.047828	4.577338
230.924503	7213.328776	8.685555	-0.047828	4.579783
231.159738	7221.427678	8.690560	-0.047878	4.582273
231.168278	7229.399533	8.695565	-0.047885	4.584723
231.345660	7237.455608	8.700570	-0.047923	4.587197
231.323643	7245.445307	8.705575	-0.047924	4.589650
231.614242	7253.504861	8.710579	-0.047984	4.592123
231.793981	7261.560919	8.715584	-0.048023	4.594593
231.851377	7269.533939	8.720589	-0.048039	4.597037
232.031553	7277.502921	8.725594	-0.048078	4.599478
232.267712	7285.547558	8.730599	-0.048127	4.601941
232.413193	7293.526263	8.735603	-0.048160	4.604382
232.410492	7301.625777	8.740608	-0.048165	4.606859
232.618652	7309.526242	8.745613	-0.048209	4.609274
232.704956	7317.600662	8.750618	-0.048231	4.611741
233.002513	7325.588400	8.755623	-0.048291	4.614180
232.947801	7333.660272	8.760627	-0.048287	4.616643
232.976092	7341.633055	8.765632	-0.048297	4.619075
232.968092	7349.644872	8.770637	-0.048301	4.621517
233.316178	7357.657075	8.775642	-0.048372	4.623958
233.692297	7365.729058	8.780647	-0.048447	4.626416
233.617607	7373.693164	8.785651	-0.048439	4.628840
233.762448	7381.757176	8.790656	-0.048471	4.631293
233.951995	7389.743422	8.795661	-0.048512	4.633721
234.298520	7397.805109	8.800666	-0.048582	4.636171
234.102385	7405.750922	8.805671	-0.048551	4.638584
234.146716	7413.751706	8.810675	-0.048564	4.641013
234.591179	7421.795689	8.815680	-0.048652	4.643453
234.635958	7429.765870	8.820685	-0.048666	4.645869
234.809965	7437.805482	8.825690	-0.048704	4.648306
234.865608	7445.837712	8.830695	-0.048720	4.650739
234.914247	7453.857654	8.835699	-0.048734	4.653167
235.338982	7461.917079	8.840704	-0.048819	4.655605
235.330447	7469.872036	8.845709	-0.048823	4.658011
235.561642	7477.905325	8.850714	-0.048871	4.660439
235.535311	7485.885072	8.855719	-0.048872	4.662850
235.522038	7493.906230	8.860723	-0.048875	4.665272
235.719055	7501.943822	8.865728	-0.048917	4.667697
235.743330	7509.948687	8.870733	-0.048927	4.670112
235.973284	7518.089168	8.875738	-0.048975	4.672566
236.032707	7526.111957	8.880743	-0.048992	4.674983
236.264509	7534.046465	8.885747	-0.049040	4.677372
236.235237	7542.042913	8.890752	-0.049040	4.679779
236.389362	7549.999825	8.895757	-0.049074	4.682173
236.668905	7558.021805	8.900762	-0.049132	4.684585
236.650600	7566.058793	8.905767	-0.049134	4.687000
236.795637	7574.052038	8.910771	-0.049166	4.689401
236.948898	7582.091099	8.915776	-0.049200	4.691814
236.940710	7590.104206	8.920781	-0.049204	4.694219
236.808416	7598.156019	8.925786	-0.049185	4.696634
236.887760	7606.100847	8.930791	-0.049205	4.699016
237.204934	7614.157699	8.935795	-0.049270	4.701429
237.275598	7622.134688	8.940800	-0.049288	4.703818
237.601182	7630.161448	8.945805	-0.049354	4.706219
237.766729	7638.155752	8.950810	-0.049390	4.708610
237.637995	7646.208326	8.955815	-0.049372	4.711018
237.783091	7654.259824	8.960819	-0.049404	4.713424
238.111762	7662.287709	8.965824	-0.049471	4.715821
238.298514	7670.233911	8.970829	-0.049511	4.718193
238.616583	7678.266935	8.975834	-0.049576	4.720589
238.623052	7686.306707	8.980839	-0.049582	4.722987
238.741998	7694.299191	8.985843	-0.049610	4.725369
238.973840	7702.386926	8.990848	-0.049659	4.727778
238.974955	7710.332028	8.995853	-0.049664	4.730144
239.192142	7718.422705	9.000858	-0.049710	4.732551
239.348158	7726.400479	9.005863	-0.049745	4.734924
239.299669	7734.363508	9.010867	-0.049741	4.737292
239.624432	7742.415166	9.015872	-0.049807	4.739683
239.833846	7750.436202	9.020877	-0.049851	4.742065
239.821472	7758.425388	9.025882	-0.049855	4.744437
240.079525	7766.464595	9.030887	-0.049908	4.746822
240.307909	7774.447611	9.035891	-0.049956	4.749188
240.335270	7782.573664	9.040896	-0.049967	4.751597
240.198447	7790.579752	9.045901	-0.049947	4.753969
240.524108	7798.606664	9.050906	-0.050013	4.756345
240.512850	7806.531475	9.055911	-0.050016	4.758691
240.708362	7814.504860	9.060915	-0.050058	4.761049
240.832881	7822.559585	9.065920	-0.050086	4.763430
241.029505	7830.522060	9.070925	-0.050128	4.765782
241.203157	7838.513641	9.075930	-0.050166	4.768142
241.277899	7846.568305	9.080935	-0.050185	4.770520
241.657980	7854.623510	9.085939	-0.050262	4.772896
241.848058	7862.697365	9.090944	-0.050303	4.775276
241.972026	7870.639924	9.095949	-0.050331	4.777617
242.061627	7878.670765	9.100954	-0.050353	4.779983
242.133029	7886.684173	9.105959	-0.050372	4.782342
242.026278	7894.631231	9.110963	-0.050357	4.784682
242.274118	7902.751604	9.115968	-0.050409	4.787070
242.345394	7910.688861	9.120973	-0.050428	4.789404
242.731816	7918.766283	9.125978	-0.050505	4.791776
242.732804	7926.769988	9.130983	-0.050511	4.794127
243.029082	7934.771337	9.135987	-0.050571	4.796475
243.072201	7942.781469	9.140992	-0.050585	4.798826
242.857472	7950.800179	9.145997	-0.050550	4.801179
243.265258	7958.784333	9.151002	-0.050632	4.803518
243.469492	7966.810953	9.156007	-0.050675	4.805869
243.606531	7974.813881	9.161011	-0.050706	4.808213
243.816545	7982.865668	9.166016	-0.050751	4.810569
243.893295	7990.226729	9.171021	-0.050770	4.812722
243.988606	7994.822116	9.176026	-0.050791	4.814066

243.908170	7997.309341	9.181031	-0.050778	4.814794
243.925612	7998.501184	9.186035	-0.050782	4.815142
243.918170	7999.055242	9.191040	-0.050781	4.815304
243.800146	7999.886217	9.196045	-0.050760	4.815548
243.855680	7999.903157	9.201050	-0.050770	4.815552
243.914873	7999.862494	9.206055	-0.050782	4.815540
243.992992	7999.886208	9.211059	-0.050796	4.815547
244.202693	7999.868285	9.216064	-0.050836	4.815541
244.144446	7999.803285	9.221069	-0.050825	4.815522
244.309830	7999.872202	9.226074	-0.050856	4.815541
244.412267	7999.782055	9.231079	-0.050875	4.815514
244.524254	7999.710217	9.236083	-0.050896	4.815493
244.636223	7999.838062	9.241088	-0.050917	4.815530
244.418344	7999.804633	9.246093	-0.050877	4.815521
244.548366	7999.864432	9.251098	-0.050901	4.815538
244.672617	7999.858999	9.256103	-0.050925	4.815536
244.505448	7999.858430	9.261107	-0.050894	4.815536
244.712204	7999.903462	9.266112	-0.050933	4.815548
244.598611	7999.880273	9.271117	-0.050912	4.815542
244.677744	7999.853816	9.276122	-0.050927	4.815534
244.766214	7999.861683	9.281127	-0.050943	4.815536
244.793926	7999.840796	9.286131	-0.050949	4.815530
245.123325	7999.913454	9.291136	-0.051010	4.815549
244.860851	7999.859008	9.296141	-0.050962	4.815535
245.047335	7999.865267	9.301146	-0.050996	4.815536
245.234645	7999.852319	9.306151	-0.051032	4.815531
244.994776	7999.836684	9.311155	-0.050987	4.815528
245.077853	7999.903194	9.316160	-0.051003	4.815547
245.180548	7999.903817	9.321165	-0.051022	4.815546
245.406226	7999.902173	9.326170	-0.051064	4.815545
245.372357	7999.878147	9.331175	-0.051058	4.815538
245.095303	7999.880059	9.336179	-0.051007	4.815540
245.234483	7999.890887	9.341184	-0.051033	4.815542
245.088192	7999.838334	9.346189	-0.051006	4.815528
245.264130	7999.856168	9.351194	-0.051039	4.815532
245.217458	7999.844748	9.356199	-0.051030	4.815529
245.100709	7999.794811	9.361203	-0.051009	4.815515
245.201646	7999.863748	9.366208	-0.051028	4.815534
245.192203	7999.866816	9.371213	-0.051026	4.815535
245.314946	7999.895530	9.376218	-0.051049	4.815543
245.358998	7999.854620	9.381223	-0.051058	4.815531
245.208339	7999.807334	9.386227	-0.051030	4.815518
245.478990	7999.868358	9.391232	-0.051081	4.815534
245.416005	7999.824636	9.396237	-0.051069	4.815522
245.674564	7999.852360	9.401242	-0.051117	4.815529
245.453945	7999.868005	9.406247	-0.051077	4.815534
245.534878	7999.866138	9.411251	-0.051092	4.815533
245.445225	7999.919157	9.416256	-0.051075	4.815549
245.496817	7999.864487	9.421261	-0.051085	4.815533
245.640795	7999.859376	9.426266	-0.051112	4.815531
245.554671	7999.914588	9.431271	-0.051096	4.815547
245.552167	7999.844087	9.436275	-0.051096	4.815527
245.651251	7999.910859	9.441280	-0.051115	4.815546
245.677088	7999.871788	9.446285	-0.051120	4.815534
245.850791	7999.899197	9.451290	-0.051152	4.815542
245.738642	7999.822638	9.456295	-0.051132	4.815520
245.870498	7999.904894	9.461299	-0.051156	4.815543
245.730581	7999.962433	9.466304	-0.051131	4.815561
245.566880	7999.891441	9.471309	-0.051100	4.815541
245.815039	7999.926471	9.476314	-0.051147	4.815550
245.811139	7999.910408	9.481319	-0.051146	4.815545
245.922966	7999.914384	9.486323	-0.051167	4.815546
246.038037	7999.956857	9.491328	-0.051189	4.815557
246.006806	7999.890158	9.496333	-0.051183	4.815538
245.791670	7999.911232	9.501338	-0.051143	4.815545
245.968910	7999.923749	9.506343	-0.051177	4.815548
245.889529	7999.871216	9.511347	-0.051162	4.815533
245.984474	7999.930447	9.516352	-0.051180	4.815550
245.626479	7999.861628	9.521357	-0.051114	4.815532
245.929464	7999.861243	9.526362	-0.051170	4.815530
245.834885	7999.884282	9.531367	-0.051153	4.815537
246.015662	7999.829581	9.536371	-0.051187	4.815520
245.946233	7999.867979	9.541376	-0.051174	4.815532
246.069010	7999.879609	9.546381	-0.051197	4.815535
246.182872	7999.923130	9.551386	-0.051218	4.815547
246.120935	7999.886899	9.556391	-0.051207	4.815537
246.319346	7999.853843	9.561395	-0.051244	4.815526
246.018026	7999.909820	9.566400	-0.051188	4.815544
245.955355	7999.858627	9.571405	-0.051177	4.815529
246.082686	7999.848974	9.576410	-0.051201	4.815526
245.983030	7999.855911	9.581415	-0.051182	4.815528
246.050060	7999.874108	9.586419	-0.051195	4.815533
246.242340	7999.833477	9.591424	-0.051231	4.815520
246.041541	7999.860123	9.596429	-0.051194	4.815529
245.849503	7999.846334	9.601434	-0.051158	4.815526
246.030501	7999.855709	9.606439	-0.051192	4.815528
246.161541	7999.849319	9.611443	-0.051217	4.815525
246.235539	7999.897530	9.616448	-0.051231	4.815539
246.132349	7999.828591	9.621453	-0.051212	4.815519
246.393505	7999.802965	9.626458	-0.051261	4.815511
246.254029	7999.869054	9.631463	-0.051235	4.815531
246.242899	7999.860348	9.636467	-0.051233	4.815528
246.239220	7999.878460	9.641472	-0.051233	4.815533
246.243962	7999.863606	9.646477	-0.051234	4.815529
246.170457	7999.913684	9.651482	-0.051220	4.815544
246.294697	7999.889031	9.656487	-0.051244	4.815536
246.285969	7999.860074	9.661491	-0.051242	4.815528
246.328808	7999.896031	9.666496	-0.051250	4.815538
246.176305	7999.836966	9.671501	-0.051222	4.815522
246.242156	7999.840193	9.676506	-0.051235	4.815522
246.262885	7999.898215	9.681511	-0.051239	4.815539
246.171615	7999.881795	9.686515	-0.051222	4.815535
246.240939	7999.903233	9.691520	-0.051235	4.815541
245.973267	7999.874328	9.696525	-0.051185	4.815533
246.130145	7999.851274	9.701530	-0.051215	4.815526
246.159545	7999.887011	9.706535	-0.051221	4.815536
246.240654	7999.857383	9.711539	-0.051236	4.815527
246.344857	7999.883661	9.716544	-0.051255	4.815534
246.067877	7999.826840	9.721549	-0.051204	4.815519
246.347132	7999.847427	9.726554	-0.051256	4.815524
246.378366	7999.905620	9.731559	-0.051262	4.815541
246.368029	7999.887316	9.736563	-0.051261	4.815535
246.507362	7999.906692	9.741568	-0.051287	4.815540
246.442989	7999.847995	9.746573	-0.051275	4.815523
246.320956	7999.900486	9.751578	-0.051253	4.815539
246.382754	7999.931413	9.756583	-0.051264	4.815548
246.283445	7999.883893	9.761587	-0.051246	4.815535
246.414631	7999.895661	9.766592	-0.051271	4.815537
246.207164	7999.911520	9.771597	-0.051232	4.815543
246.378550	7999.889770	9.776602	-0.051264	4.815536
246.193993	7999.886780	9.781607	-0.051230	4.815536
246.282134	7999.876489	9.786611	-0.051247	4.815532
246.482248	7999.940638	9.791616	-0.051284	4.815550
246.488471	7999.891635	9.796621	-0.051286	4.815536
246.371263	7999.905761	9.801626	-0.051264	4.815541
246.572862	7999.912270	9.806631	-0.051302	4.815542
246.414764	7999.894761	9.811635	-0.051272	4.815537
246.646972	7999.906039	9.816640	-0.051316	4.815539
246.570874	7999.873848	9.821645	-0.051302	4.815530
246.668079	7999.916031	9.826650	-0.051320	4.815542
246.601629	7999.904287	9.831655	-0.051308	4.815539
246.444810	7999.895342	9.836659	-0.051279	4.815537
246.521309	7999.932916	9.841664	-0.051294	4.815548
246.626466	7999.911155	9.846669	-0.051313	4.815541
246.538362	7999.851003	9.851674	-0.051297	4.815524
246.660274	7999.892520	9.856679	-0.051320	4.815535
246.576347	7999.836708	9.861683	-0.051305	4.815519
246.648025	7999.926530	9.866688	-0.051318	4.815545
246.530985	7999.877653	9.871693	-0.051297	4.815532
246.474152	7999.902375	9.876698	-0.051286	4.815539
246.747284	7999.913253	9.881703	-0.051337	4.815541
246.686526	7999.869565	9.886707	-0.051326	4.815528
246.767511	7999.934977	9.891712	-0.051342	4.815547
246.839653	7999.914814	9.896717	-0.051355	4.815541
246.700181	7999.852756	9.901722	-0.051329	4.815523
246.787207	7999.906520	9.906727	-0.051346	4.815539
246.846438	7999.929930	9.911731	-0.051357	4.815545
246.848282	7999.964151	9.916736	-0.051358	4.815555
246.611017	7999.900499	9.921741	-0.051314	4.815538
246.703933	7999.910576	9.926746	-0.051331	4.815540
246.948507	7999.944483	9.931751	-0.051377	4.815549
246.879916	7999.915617	9.936755	-0.051364	4.815541
246.861698	7999.933493	9.941760	-0.051361	4.815546
246.647130	7999.904384	9.946765	-0.051321	4.815539
246.740989	7999.892049	9.951770	-0.051339	4.815535
246.768230	7999.923481	9.956775	-0.051344	4.815544
246.659393	7999.881145	9.961779	-0.051324	4.815532
246.969848	7999.909718	9.966784	-0.051382	4.815539
246.836565	7999.897953	9.971789	-0.051358	4.815536
247.125206	7999.894134	9.976794	-0.051412	4.815533
246.837665	7999.935384	9.981799	-0.051358	4.815547
246.703256	7999.886223	9.986803	-0.051334	4.815533
246.784220	7999.943092	9.991808	-0.051349	4.815549
246.799432	7999.863266	9.996813	-0.051352	4.815526
246.816811	7999.882790	10.001818	-0.051355	4.815532
246.795899	7999.914505	10.006823	-0.051352	4.815541
246.675950	7999.858105	10.011827	-0.051329	4.815525
246.923402	7999.878176	10.016832	-0.051376	4.815530
246.698797	7999.872397	10.021837	-0.051334	4.815529
246.683820	7999.870035	10.026842	-0.051332	4.815528
246.801571	7999.880516	10.031847	-0.051354	4.815531
246.769734	7999.882151	10.036851	-0.051348	4.815532
246.996048	7999.908285	10.041856	-0.051390	4.815538
246.887368	7999.888377	10.046861	-0.051370	4.815533
247.121444	7999.890076	10.051866	-0.051414	4.815532
247.082358	7999.889457	10.056871	-0.051407	4.815532
247.031686	7999.875835	10.061875	-0.051398	4.815528
246.918066	7999.897495	10.066880	-0.051377	4.815535
246.821770	7999.857499	10.071885	-0.051359	4.815524
246.957144	7999.870403	10.076890	-0.051385	4.815527
246.753108	7999.893792	10.081895	-0.051347	4.815535
246.844639	7999.835501	10.086899	-0.051364	4.815518
246.810362	7999.905442	10.091904	-0.051358	4.815538
246.998448	7999.918138	10.096909	-0.051393	4.815541
247.082128	7999.894959	10.101914	-0.051409	4.815534
247.167716	7999.917731	10.106919	-0.051425	4.815540
246.861011	7999.873236	10.111923	-0.051368	4.815528
246.913393	7999.892263	10.116928	-0.051378	4.815534
246.905908	7999.875073	10.121933	-0.051377	4.815529
246.957384	7999.890881	10.126938	-0.051387	4.815533
246.977129	7999.893357	10.131943	-0.051391	4.815534
247.236597	7999.893334	10.136947	-0.051439	4.815532
247.124823	7999.934246	10.141952	-0.051419	4.815545
247.132157	7999.889532	10.146957	-0.051420	4.815532
247.241346	7999.913757	10.151962	-0.051441	4.815538
247.089205	7999.908091	10.156967	-0.051413	4.815537
246.829609	7999.824853	10.161971	-0.051364	4.815514
246.944449	7999.896156	10.166976	-0.051386	4.815535
246.906108	7999.914772	10.171981	-0.051379	4.815540
246.821705	7999.919821	10.176986	-0.051364	4.815542
246.968774	7999.914762	10.181991	-0.051391	4.815540
246.924325	7999.882019	10.186995	-0.051383	4.815531
246.962265	7999.925372	10.192000	-0.051390	4.815543
247.044732	7999.889358	10.197005	-0.051406	4.815532
247.110441	7999.903263	10.202010	-0.051418	4.815536
247.182976	7999.898057	10.207015	-0.051432	4.815534
247.008684	7999.851449	10.212019	-0.051400	4.815521
247.281801	7999.903976	10.217024	-0.051451	4.815535
247.222727	7999.873130	10.222029	-0.051440	4.815527
247.057488	7999.844825	10.227034	-0.051410	4.815519
247.295195	7999.902114	10.232039	-0.051454	4.815535
247.314546	7999.889633	10.237043	-0.051458	4.815531
247.204478	7999.877178	10.242048	-0.051438	4.815528
246.872631	7999.852563	10.247053	-0.051376	4.815522
247.064901	7999.859988	10.252058	-0.051412	4.815523
247.276283	7999.900830	10.257063	-0.051452	4.815534
247.161230	7999.838102	10.262067	-0.051430	4.815517
247.233054	7999.893754	10.267072	-0.051444	4.815532
247.112514	7999.871517	10.272077	-0.051422	4.815527
247.051858	7999.955979	10.277082	-0.051411	4.815552
247.056535	7999.981703	10.282087	-0.051412	4.815559
246.988487	7999.947507	10.287091	-0.051399	4.815549
247.072077	7999.964907	10.292096	-0.051415	4.815554
246.929150	7999.901724	10.297101	-0.051389	4.815536
247.003497	7999.888004	10.302106	-0.051403	4.815532
247.004166	7999.898712	10.307111	-0.051403	4.815535
246.847022	7999.825687	10.312115	-0.051374	4.815514
247.230398	7999.918456	10.317120	-0.051446	4.815540
247.209736	7999.856199	10.322125	-0.051442	4.815522
247.188692	7999.865486	10.327130	-0.051438	4.815524
247.097227	7999.919544	10.332135	-0.051421	4.815541
247.254004	7999.872995	10.337139	-0.051451	4.815526
247.046906	7999.902741	10.342144	-0.051412	4.815536
246.949398	7999.887287	10.347149	-0.051394	4.815532
247.082597	7999.877730	10.352154	-0.051419	4.815528
247.144953	7999.899056	10.357159	-0.051431	4.815534
246.885649	7999.852130	10.362163	-0.051383	4.815522
246.900566	7999.871614	10.367168	-0.051386	4.815528
246.950164	7999.907682	10.372173	-0.051396	4.815538
247.122939	7999.893431	10.377178	-0.051428	4.815533
247.224145	7999.900439	10.382183	-0.051447	4.815534
247.160740	7999.849232	10.387187	-0.051435	4.815520
247.304838	7999.959459	10.392192	-0.051463	4.815551
247.046122	7999.969141	10.397197	-0.051415	4.815555
247.192846	7999.912817	10.402202	-0.051442	4.815538
247.090405	7999.891943	10.407207	-0.051423	4.815532
247.089663	7999.864183	10.412211	-0.051423	4.815524
246.964812	7999.853623	10.417216	-0.051400	4.815522
247.037311	7999.993651	10.422221	-0.051414	4.815562
246.931295	7999.871268	10.427226	-0.051394	4.815527
246.929446	7999.905429	10.432231	-0.051394	4.815537
247.166658	7999.864463	10.437235	-0.051439	4.815524
247.319041	7999.897935	10.442240	-0.051467	4.815533
247.048974	7999.902093	10.447245	-0.051417	4.815536
246.874450	7999.884315	10.452250	-0.051385	4.815531
247.016658	7999.898399	10.457255	-0.051412	4.815535
247.003133	7999.937709	10.462259	-0.051409	4.815546
247.109873	7999.935197	10.467264	-0.051429	4.815545
247.111134	7999.896791	10.472269	-0.051430	4.815534
247.118132	7999.925757	10.477274	-0.051431	4.815542
246.958144	7999.909284	10.482279	-0.051402	4.815538
247.009714	7999.861020	10.487283	-0.051412	4.815524
247.138715	7999.958185	10.492288	-0.051436	4.815552
247.183242	7999.953590	10.497293	-0.051444	4.815550
247.046763	7999.941772	10.502298	-0.051419	4.815547
247.015140	7999.934867	10.507303	-0.051413	4.815545
247.041430	7999.878715	10.512307	-0.051419	4.815529
247.234392	7999.957701	10.517312	-0.051455	4.815551
246.956866	7999.907274	10.522317	-0.051403	4.815537
247.221937	7999.953263	10.527322	-0.051453	4.815550
247.103904	7999.940678	10.532327	-0.051431	4.815547
246.938516	7999.932660	10.537331	-0.051400	4.815545
247.079496	7999.945656	10.542336	-0.051427	4.815548
247.086554	7999.905209	10.547341	-0.051428	4.815536
246.912932	7999.899193	10.552346	-0.051396	4.815535
247.252128	7999.912217	10.557351	-0.051460	4.815537
247.190756	7999.901624	10.562355	-0.051448	4.815535
247.107244	7999.906688	10.567360	-0.051433	4.815537
247.029339	7999.934269	10.572365	-0.051419	4.815545
247.122337	7999.928329	10.577370	-0.051436	4.815543
247.056605	7999.943294	10.582375	-0.051424	4.815547
246.931313	7999.939134	10.587379	-0.051401	4.815547
247.144821	7999.986418	10.592384	-0.051441	4.815560
247.149341	7999.929911	10.597389	-0.051442	4.815543
247.019180	7999.902177	10.602394	-0.051418	4.815536
247.183505	7999.929437	10.607399	-0.051449	4.815543
247.012967	7999.843378	10.612403	-0.051417	4.815518
247.091000	7999.988836	10.617408	-0.051432	4.815561
247.142944	7999.901065	10.622413	-0.051442	4.815535
247.374734	7999.964666	10.627418	-0.051485	4.815552
247.359083	7999.960158	10.632423	-0.051483	4.815551
247.147966	7999.955665	10.637427	-0.051444	4.815551
247.221556	7999.940865	10.642432	-0.051458	4.815546
247.296771	7999.941042	10.647437	-0.051472	4.815546
247.110312	7999.889964	10.652442	-0.051437	4.815532
247.196182	7999.922352	10.657447	-0.051453	4.815541
247.212640	7999.898076	10.662451	-0.051457	4.815533
247.018073	7999.903465	10.667456	-0.051421	4.815536
247.211353	7999.906635	10.672461	-0.051457	4.815536
247.018719	7999.890698	10.677466	-0.051421	4.815532
247.057603	7999.919116	10.682471	-0.051429	4.815540
246.946876	7999.892767	10.687475	-0.051408	4.815533
247.294949	7999.914480	10.692480	-0.051473	4.815538
247.274575	7999.926981	10.697485	-0.051470	4.815542
247.298710	7999.932732	10.702490	-0.051474	4.815543
247.292539	7999.951872	10.707495	-0.051474	4.815549
247.231354	7999.917788	10.712499	-0.051462	4.815539
247.247857	7999.940501	10.717504	-0.051466	4.815546
247.362757	7999.942394	10.722509	-0.051487	4.815546
247.187323	7999.922464	10.727514	-0.051455	4.815541
247.278320	7999.957072	10.732519	-0.051472	4.815550
247.107262	7999.944690	10.737523	-0.051440	4.815547
247.128589	7999.943988	10.742528	-0.051444	4.815547
247.210349	7999.930389	10.747533	-0.051460	4.815543
247.066151	7999.976112	10.752538	-0.051433	4.815557
247.060627	7999.974972	10.757543	-0.051432	4.815557
247.234741	7999.899872	10.762547	-0.051465	4.815534
247.406881	7999.932599	10.767552	-0.051497	4.815542
247.205711	7999.885553	10.772557	-0.051460	4.815530
247.110392	7999.873338	10.777562	-0.051443	4.815527
247.428653	7999.969319	10.782567	-0.051502	4.815553
247.252895	7999.945112	10.787571	-0.051470	4.815547
247.191897	7999.917438	10.792576	-0.051458	4.815539
247.279869	7999.932774	10.797581	-0.051475	4.815543
247.113961	7999.908729	10.802586	-0.051444	4.815537
247.285520	7999.927563	10.807591	-0.051476	4.815542
247.258148	7999.911117	10.812595	-0.051472	4.815537
247.289932	7999.924468	10.817600	-0.051478	4.815541
247.174673	7999.920471	10.822605	-0.051456	4.815540
247.237309	7999.891610	10.827610	-0.051468	4.815531
247.265781	7999.938013	10.832615	-0.051474	4.815545
247.189612	7999.918634	10.837619	-0.051460	4.815539
247.277596	7999.960668	10.842624	-0.051476	4.815551
247.264586	7999.882517	10.847629	-0.051474	4.815528
247.149923	7999.932993	10.852634	-0.051453	4.815544
247.114400	7999.969809	10.857639	-0.051447	4.815555
247.439090	7999.972987	10.862643	-0.051507	4.815554
247.442421	7999.979467	10.867648	-0.051508	4.815556
247.448356	7999.945409	10.872653	-0.051509	4.815546
247.408080	8000.000302	10.877658	-0.051502	4.815562
247.655771	7999.959508	10.882663	-0.051549	4.815549
247.566611	7999.908948	10.887667	-0.051532	4.815535
247.526321	7999.953162	10.892672	-0.051525	4.815548
247.609203	7999.963075	10.897677	-0.051540	4.815550
247.538067	7999.950186	10.902682	-0.051527	4.815547
247.439110	7999.951794	10.907687	-0.051509	4.815548
247.472208	7999.949149	10.912691	-0.051516	4.815547
247.363925	7999.980506	10.917696	-0.051496	4.815557
247.267966	7999.964009	10.922701	-0.051478	4.815552
247.303638	7999.966745	10.927706	-0.051485	4.815553
247.418432	7999.983586	10.932711	-0.051506	4.815557
247.495477	7999.925058	10.937715	-0.051521	4.815540
247.484216	7999.961202	10.942720	-0.051519	4.815550
247.373740	7999.967962	10.947725	-0.051499	4.815553
247.594669	7999.953429	10.952730	-0.051540	4.815547
247.239013	7999.987160	10.957735	-0.051474	4.815559
247.472475	7999.917299	10.962739	-0.051518	4.815537
247.685743	7999.980600	10.967744	-0.051558	4.815555
247.439675	7999.842047	10.972749	-0.051512	4.815516
247.552437	7999.840700	10.977754	-0.051533	4.815515
247.581363	7999.914877	10.982759	-0.051539	4.815536
247.643135	7999.983182	10.987763	-0.051551	4.815556
247.518362	7999.882917	10.992768	-0.051527	4.815527
247.489654	7999.903825	10.997773	-0.051522	4.815533
247.452102	7999.876533	11.002778	-0.051516	4.815526
247.454674	7999.950280	11.007783	-0.051516	4.815547
247.424419	7999.911360	11.012787	-0.051511	4.815536
247.645457	7999.933138	11.017792	-0.051552	4.815541
247.713131	7999.954551	11.022797	-0.051565	4.815547
247.769259	7999.921311	11.027802	-0.051576	4.815537
247.867358	7999.962443	11.032807	-0.051594	4.815549
247.672824	7999.913367	11.037811	-0.051558	4.815535
247.759700	7999.942569	11.042816	-0.051575	4.815543
247.854173	7999.949468	11.047821	-0.051592	4.815545
247.773636	7999.957784	11.052826	-0.051578	4.815548
247.690435	7999.956445	11.057831	-0.051562	4.815548
247.510399	7999.949255	11.062835	-0.051529	4.815547
247.587103	7999.890721	11.067840	-0.051543	4.815529
247.571744	7999.937477	11.072845	-0.051541	4.815543
247.482379	7999.938174	11.077850	-0.051524	4.815543
247.609848	7999.933864	11.082855	-0.051548	4.815542
247.580384	7999.901364	11.087859	-0.051543	4.815532
247.463658	7999.912294	11.092864	-0.051522	4.815536
247.663019	7999.914496	11.097869	-0.051559	4.815536
247.451248	7999.865140	11.102874	-0.051520	4.815522
247.619401	7999.958674	11.107879	-0.051551	4.815549
247.490314	7999.953383	11.112883	-0.051527	4.815548
247.586460	7999.998754	11.117888	-0.051545	4.815561
247.416222	7999.946872	11.122893	-0.051514	4.815546
247.511424	7999.887571	11.127898	-0.051532	4.815528
247.636106	7999.968649	11.132903	-0.051555	4.815552
247.593761	7999.948754	11.137907	-0.051548	4.815546
247.458330	7999.944428	11.142912	-0.051523	4.815545
247.517842	7999.932602	11.147917	-0.051534	4.815542
247.530184	7999.999033	11.152922	-0.051536	4.815561
247.587794	7999.916693	11.157927	-0.051547	4.815537
247.425201	7999.843577	11.162931	-0.051517	4.815516
247.705309	7999.949616	11.167936	-0.051570	4.815546
247.874705	7999.942787	11.172941	-0.051601	4.815543
247.737018	7999.917065	11.177946	-0.051576	4.815536
247.693856	7999.958028	11.182951	-0.051568	4.815548
247.809811	7999.935376	11.187955	-0.051590	4.815541
247.812801	7999.949326	11.192960	-0.051591	4.815545
247.703159	7999.927265	11.197965	-0.051571	4.815539
247.802976	7999.934251	11.202970	-0.051589	4.815541
247.720104	7999.995926	11.207975	-0.051574	4.815559
247.497898	7999.896206	11.212979	-0.051533	4.815531
247.684446	7999.951596	11.217984	-0.051568	4.815546
247.685351	7999.947357	11.222989	-0.051568	4.815545
247.554655	7999.907866	11.227994	-0.051544	4.815534
247.785894	7999.949034	11.232999	-0.051587	4.815545
247.675310	7999.941909	11.238003	-0.051567	4.815543
247.423296	7999.945292	11.243008	-0.051520	4.815546
247.369009	8000.021315	11.248013	-0.051510	4.815568
247.490310	7999.922928	11.253018	-0.051533	4.815539
247.513019	7999.961762	11.258023	-0.051538	4.815550
247.233689	7999.895285	11.263027	-0.051486	4.815532
247.587477	7999.916024	11.268032	-0.051552	4.815536
247.558616	7999.920911	11.273037	-0.051547	4.815538
247.435528	7999.885817	11.278042	-0.051524	4.815528
247.580490	7999.943731	11.283047	-0.051551	4.815544
247.534671	7999.935527	11.288051	-0.051543	4.815542
247.665229	7999.984664	11.293056	-0.051567	4.815556
247.718689	7999.965263	11.298061	-0.051578	4.815550
247.736906	7999.969851	11.303066	-0.051581	4.815551
247.553532	7999.980761	11.308071	-0.051547	4.815555
247.642309	7999.945918	11.313075	-0.051564	4.815545
247.724009	7999.964356	11.318080	-0.051579	4.815550
247.549205	7999.959387	11.323085	-0.051547	4.815549
247.284893	7999.920921	11.328090	-0.051498	4.815539
247.440143	7999.921335	11.333095	-0.051527	4.815538
247.437347	7999.911697	11.338099	-0.051527	4.815536
247.554653	7999.937123	11.343104	-0.051549	4.815542
247.644478	7999.977052	11.348109	-0.051566	4.815554
247.606106	7999.914505	11.353114	-0.051559	4.815536
247.724026	7999.944213	11.358119	-0.051581	4.815544
247.460302	7999.939929	11.363123	-0.051532	4.815544
247.618220	7999.941455	11.368128	-0.051562	4.815543
247.626101	7999.935195	11.373133	-0.051564	4.815542
247.508076	7999.905522	11.378138	-0.051542	4.815533
247.541492	7999.946667	11.383143	-0.051548	4.815545
247.523768	7999.920766	11.388147	-0.051545	4.815538
247.559747	7999.940594	11.393152	-0.051552	4.815543
247.622739	7999.929892	11.398157	-0.051564	4.815540
247.578462	7999.862977	11.403162	-0.051556	4.815521
247.571729	7999.900263	11.408167	-0.051555	4.815532
247.563365	7999.954609	11.413171	-0.051554	4.815547
247.611544	7999.887066	11.418176	-0.051563	4.815528
247.637251	7999.892843	11.423181	-0.051568	4.815529
247.507591	7999.893951	11.428186	-0.051544	4.815530
247.586005	7999.930490	11.433191	-0.051559	4.815540
247.688079	7999.906543	11.438195	-0.051578	4.815533
247.849605	7999.970068	11.443200	-0.051608	4.815551
247.759506	7999.948326	11.448205	-0.051592	4.815545
247.722561	7999.919975	11.453210	-0.051585	4.815537
247.844747	7999.958297	11.458215	-0.051608	4.815547
247.649097	7999.891048	11.463219	-0.051572	4.815528
247.929302	7999.909520	11.468224	-0.051624	4.815532
247.853746	7999.991605	11.473229	-0.051610	4.815557
247.856145	7999.935062	11.478234	-0.051611	4.815540
247.812175	7999.945042	11.483239	-0.051603	4.815543
247.782153	7999.937095	11.488243	-0.051597	4.815541
247.657172	7999.956433	11.493248	-0.051574	4.815547
247.564891	7999.921841	11.498253	-0.051557	4.815538
247.698880	7999.903754	11.503258	-0.051583	4.815532
247.638938	7999.963667	11.508263	-0.051572	4.815550
247.439325	7999.928391	11.513267	-0.051535	4.815540
247.561432	7999.921858	11.518272	-0.051558	4.815538
247.839919	7999.944574	11.523277	-0.051610	4.815543
247.922106	7999.921370	11.528282	-0.051625	4.815536
247.744012	7999.935570	11.533287	-0.051592	4.815541
247.831696	7999.913525	11.538291	-0.051609	4.815534
247.844749	7999.926571	11.543296	-0.051611	4.815538
247.664833	7999.900160	11.548301	-0.051578	4.815531
247.566449	7999.887895	11.553306	-0.051560	4.815528
247.607922	7999.947325	11.558311	-0.051568	4.815545
247.434472	7999.959466	11.563315	-0.051536	4.815549
247.558428	7999.926264	11.568320	-0.051559	4.815539
247.563072	7999.909272	11.573325	-0.051560	4.815534
247.639694	7999.896657	11.578330	-0.051575	4.815530
247.667260	7999.947317	11.583335	-0.051580	4.815545
247.760416	7999.918953	11.588339	-0.051598	4.815536
248.114208	7999.953578	11.593344	-0.051664	4.815544
247.891354	7999.918990	11.598349	-0.051622	4.815535
248.007930	7999.905959	11.603354	-0.051644	4.815531
248.123679	7999.964467	11.608359	-0.051666	4.815547
248.069548	7999.928360	11.613363	-0.051656	4.815537
247.871474	7999.992427	11.618368	-0.051620	4.815557
247.995231	7999.993396	11.623373	-0.051643	4.815557
247.876335	7999.935942	11.628378	-0.051621	4.815540
247.998973	7999.949709	11.633383	-0.051644	4.815544
247.944977	7999.964865	11.638387	-0.051634	4.815548
247.899507	7999.962006	11.643392	-0.051626	4.815548
247.925415	7999.954972	11.648397	-0.051631	4.815546
247.768106	7999.899027	11.653402	-0.051602	4.815530
247.951099	7999.974650	11.658407	-0.051636	4.815551
247.770269	7999.947156	11.663411	-0.051603	4.815544
247.796178	7999.962548	11.668416	-0.051608	4.815548
247.965401	7999.945036	11.673421	-0.051639	4.815542
247.919130	7999.938960	11.678426	-0.051631	4.815541
247.910470	7999.973011	11.683431	-0.051630	4.815551
247.767581	7999.891672	11.688435	-0.051603	4.815528
247.892315	7999.957801	11.693440	-0.051627	4.815547
247.959289	7999.954640	11.698445	-0.051639	4.815545
247.763037	7999.932234	11.703450	-0.051603	4.815540
248.014040	7999.955570	11.708455	-0.051650	4.815545
247.926658	7999.965910	11.713459	-0.051634	4.815549
247.995975	7999.996962	11.718464	-0.051647	4.815557
247.837360	7999.962354	11.723469	-0.051618	4.815548
247.842445	7999.924010	11.728474	-0.051619	4.815537
247.904880	7999.975240	11.733479	-0.051631	4.815552
247.826963	7999.946221	11.738483	-0.051616	4.815543
247.943299	7999.956680	11.743488	-0.051638	4.815546
247.930855	7999.956496	11.748493	-0.051636	4.815546
247.769295	7999.932520	11.753498	-0.051606	4.815540
248.058284	7999.986378	11.758503	-0.051660	4.815554
247.914245	7999.941329	11.763507	-0.051634	4.815542
247.935345	7999.960914	11.768512	-0.051638	4.815547
247.930000	7999.945894	11.773517	-0.051637	4.815543
247.987824	7999.922294	11.778522	-0.051648	4.815536
248.018553	7999.975142	11.783527	-0.051654	4.815551
247.965055	7999.945454	11.788531	-0.051644	4.815542
248.043795	7999.948892	11.793536	-0.051659	4.815543
248.080901	7999.991166	11.798541	-0.051666	4.815555
247.979968	7999.966043	11.803546	-0.051647	4.815548
248.016725	7999.988020	11.808551	-0.051655	4.815555
247.844668	7999.969212	11.813555	-0.051623	4.815550
247.826697	7999.953986	11.818560	-0.051620	4.815546
247.775987	7999.951041	11.823565	-0.051610	4.815545
247.845460	7999.929766	11.828570	-0.051623	4.815538
248.036989	7999.969219	11.833575	-0.051659	4.815549
247.991444	7999.957815	11.838579	-0.051651	4.815546
248.051397	7999.991918	11.843584	-0.051662	4.815556
248.100059	7999.966032	11.848589	-0.051672	4.815548
248.107521	7999.974715	11.853594	-0.051673	4.815550
248.185546	8000.002706	11.858599	-0.051688	4.815558
248.085833	7999.980806	11.863603	-0.051670	4.815552
248.144065	7999.990318	11.868608	-0.051681	4.815555
248.157728	7999.986288	11.873613	-0.051684	4.815553
248.134607	7999.997676	11.878618	-0.051679	4.815557
248.119379	8000.007058	11.883623	-0.051677	4.815560
248.057872	7999.982578	11.888627	-0.051666	4.815553
248.161256	7999.973603	11.893632	-0.051685	4.815550
248.294441	7999.975795	11.898637	-0.051710	4.815550
248.052041	7999.949431	11.903642	-0.051665	4.815543
248.213559	8000.000143	11.908647	-0.051695	4.815557
248.082230	7999.946757	11.913651	-0.051671	4.815542
248.167202	8000.033597	11.918656	-0.051687	4.815567
248.137460	7999.915657	11.923661	-0.051682	4.815533
247.991914	7999.972037	11.928666	-0.051655	4.815550
248.147568	7999.984207	11.933671	-0.051684	4.815553
248.097883	7999.927881	11.938675	-0.051675	4.815537
248.235480	7999.979270	11.943680	-0.051701	4.815551
248.238276	7999.951568	11.948685	-0.051702	4.815543
248.030605	7999.920431	11.953690	-0.051663	4.815535
248.128102	7999.961554	11.958695	-0.051682	4.815546
248.150317	7999.946984	11.963699	-0.051686	4.815542
248.033658	7999.923740	11.968704	-0.051664	4.815536
247.967605	7999.925884	11.973709	-0.051652	4.815537
248.080539	7999.957648	11.978714	-0.051674	4.815545
248.306591	7999.961355	11.983719	-0.051716	4.815545
247.875155	7999.939382	11.988723	-0.051636	4.815541
247.954737	7999.994096	11.993728	-0.051651	4.815557
248.175674	7999.962477	11.998733	-0.051692	4.815546
248.062840	7999.931820	12.003738	-0.051671	4.815538
248.038241	7999.953864	12.008743	-0.051667	4.815544
248.197944	7999.946877	12.013747	-0.051697	4.815542
248.195608	7999.977827	12.018752	-0.051697	4.815551
248.160793	7999.984753	12.023757	-0.051690	4.815553
248.035586	7999.918652	12.028762	-0.051667	4.815534
248.124461	7999.960702	12.033767	-0.051684	4.815546
248.073163	7999.975903	12.038771	-0.051675	4.815551
248.066359	7999.973674	12.043776	-0.051674	4.815550
248.260586	7999.968318	12.048781	-0.051710	4.815547
248.224823	7999.953870	12.053786	-0.051704	4.815543
248.017423	7999.995358	12.058791	-0.051665	4.815557
248.074202	7999.948245	12.063795	-0.051676	4.815542
248.130435	7999.937434	12.068800	-0.051687	4.815539
248.173615	7999.950972	12.073805	-0.051695	4.815543
248.148342	7999.948442	12.078810	-0.051690	4.815542
248.410442	7999.990116	12.083815	-0.051739	4.815553
248.135794	7999.963225	12.088819	-0.051688	4.815547
247.944804	7999.986826	12.093824	-0.051653	4.815554
248.286043	7999.984937	12.098829	-0.051717	4.815552
248.418082	7999.984974	12.103834	-0.051742	4.815552
248.311158	8000.009946	12.108839	-0.051722	4.815559
248.279976	7999.974214	12.113843	-0.051716	4.815549
248.352668	7999.991438	12.118848	-0.051730	4.815554
248.135795	7999.969762	12.123853	-0.051690	4.815548
247.967421	7999.954218	12.128858	-0.051659	4.815545
248.143587	8000.011576	12.133863	-0.051692	4.815561
247.961766	8000.035326	12.138867	-0.051658	4.815568
247.887149	7999.983933	12.143872	-0.051644	4.815554
247.997872	8000.003913	12.148877	-0.051665	4.815559
248.055804	7999.934393	12.153882	-0.051676	4.815538
248.082779	7999.974365	12.158887	-0.051682	4.815550
248.036511	7999.929843	12.163891	-0.051673	4.815537
248.279584	7999.973342	12.168896	-0.051719	4.815549
248.192030	7999.972999	12.173901	-0.051703	4.815549
248.195925	7999.930363	12.178906	-0.051703	4.815537
248.484929	7999.987427	12.183911	-0.051757	4.815552
248.287932	7999.938309	12.188915	-0.051721	4.815538
248.076377	7999.939147	12.193920	-0.051682	4.815540
248.164503	7999.955555	12.198925	-0.051698	4.815544
248.191485	7999.918635	12.203930	-0.051704	4.815533
248.277984	7999.965987	12.208935	-0.051720	4.815547
248.023309	7999.951170	12.213939	-0.051673	4.815543
248.210077	7999.980935	12.218944	-0.051708	4.815551
248.357101	7999.981216	12.223949	-0.051735	4.815551
248.180459	8000.014663	12.228954	-0.051703	4.815561
248.404592	8000.042902	12.233959	-0.051745	4.815568
248.329062	7999.990426	12.238963	-0.051731	4.815553
248.313647	7999.978445	12.243968	-0.051728	4.815550
248.206150	7999.979913	12.248973	-0.051708	4.815551
248.215098	7999.975806	12.253978	-0.051710	4.815550
248.349761	8000.019672	12.258983	-0.051735	4.815562
248.378824	8000.002009	12.263987	-0.051741	4.815557
248.288081	7999.999479	12.268992	-0.051724	4.815556
248.280948	7999.964138	12.273997	-0.051723	4.815546
248.232588	7999.940941	12.279002	-0.051714	4.815539
248.488404	7999.988920	12.284007	-0.051762	4.815552
248.488527	7999.983600	12.289011	-0.051763	4.815551
248.289543	8000.000662	12.294016	-0.051726	4.815557
248.267358	8000.006727	12.299021	-0.051722	4.815558
248.434426	7999.998792	12.304026	-0.051753	4.815555
248.197943	8000.010970	12.309031	-0.051709	4.815560
248.104282	7999.959267	12.314035	-0.051692	4.815545
248.276185	8000.036847	12.319040	-0.051724	4.815567
248.344967	8000.018765	12.324045	-0.051737	4.815562
248.193646	7999.966120	12.329050	-0.051709	4.815547
248.199548	8000.001477	12.334055	-0.051711	4.815557
248.377989	7999.992660	12.339059	-0.051744	4.815554
248.435285	8000.029924	12.344064	-0.051755	4.815564
248.643430	8000.000233	12.349069	-0.051794	4.815555
248.255660	7999.950137	12.354074	-0.051722	4.815542
248.463442	8000.001604	12.359079	-0.051761	4.815556
248.374574	7999.949978	12.364083	-0.051744	4.815541
248.413772	7999.963451	12.369088	-0.051752	4.815545
248.273267	7999.979332	12.374093	-0.051726	4.815550
248.205682	7999.939801	12.379098	-0.051714	4.815539
248.273903	8000.007146	12.384103	-0.051727	4.815558
248.535538	8000.001823	12.389107	-0.051776	4.815556
248.420107	8000.002093	12.394112	-0.051754	4.815556
248.543995	8000.003065	12.399117	-0.051777	4.815556
248.267409	7999.991094	12.404122	-0.051726	4.815554
248.413763	8000.040491	12.409127	-0.051754	4.815567
248.219909	8000.006375	12.414131	-0.051718	4.815558
248.245672	7999.988659	12.419136	-0.051723	4.815553
248.520925	7999.999577	12.424141	-0.051774	4.815555
248.319943	7999.966413	12.429146	-0.051737	4.815546
248.638451	8000.014347	12.434151	-0.051797	4.815559
248.454800	7999.992145	12.439155	-0.051763	4.815553
248.532148	8000.004105	12.444160	-0.051777	4.815556
248.480124	7999.994731	12.449165	-0.051768	4.815554
248.243832	7999.997301	12.454170	-0.051724	4.815556
248.681529	8000.026890	12.459175	-0.051806	4.815562
248.280017	7999.958414	12.464179	-0.051731	4.815544
248.290383	7999.968213	12.469184	-0.051733	4.815547
248.457347	7999.967752	12.474189	-0.051764	4.815546
248.086223	7999.929676	12.479194	-0.051696	4.815537
248.276760	7999.945619	12.484199	-0.051731	4.815540
248.330078	7999.944372	12.489203	-0.051741	4.815540
248.428945	7999.968430	12.494208	-0.051760	4.815546
248.359590	7999.992948	12.499213	-0.051747	4.815554
248.412743	8000.046164	12.504218	-0.051757	4.815569
248.460934	7999.945513	12.509223	-0.051767	4.815539
248.426780	7999.927886	12.514227	-0.051760	4.815534
248.568707	7999.984687	12.519232	-0.051787	4.815550
248.550156	7999.977995	12.524237	-0.051784	4.815548
248.222298	7999.966255	12.529242	-0.051723	4.815547
248.457579	8000.012831	12.534247	-0.051767	4.815559
248.230688	7999.956817	12.539251	-0.051725	4.815544
248.311004	7999.981641	12.544256	-0.051740	4.815551
248.387865	8000.020292	12.549261	-0.051755	4.815562
248.404750	7999.963984	12.554266	-0.051758	4.815545
248.476163	8000.010022	12.559271	-0.051772	4.815558
248.299409	7999.955894	12.564275	-0.051739	4.815543
248.456107	7999.969150	12.569280	-0.051768	4.815546
248.472191	8000.006809	12.574285	-0.051771	4.815557
248.291070	7999.980376	12.579290	-0.051738	4.815550
248.564415	7999.997671	12.584295	-0.051789	4.815554
248.260868	7999.956425	12.589299	-0.051733	4.815543
248.356733	7999.969756	12.594304	-0.051751	4.815547
248.399018	7999.991823	12.599309	-0.051759	4.815553
248.562763	7999.937912	12.604314	-0.051790	4.815537
248.548490	7999.996435	12.609319	-0.051787	4.815554
248.491552	7999.968826	12.614323	-0.051777	4.815546
248.491283	7999.978451	12.619328	-0.051777	4.815549
248.345426	7999.981429	12.624333	-0.051750	4.815550
248.306999	7999.964801	12.629338	-0.051743	4.815546
248.399185	7999.966324	12.634343	-0.051760	4.815546
248.318899	7999.955420	12.639347	-0.051746	4.815543
248.294936	7999.990290	12.644352	-0.051741	4.815553
248.289434	7999.967792	12.649357	-0.051741	4.815547
248.277316	7999.927030	12.654362	-0.051738	4.815535
248.351011	7999.994464	12.659367	-0.051752	4.815554
248.341146	7999.968691	12.664371	-0.051751	4.815547
248.398891	7999.982467	12.669376	-0.051762	4.815550
248.633300	8000.023690	12.674381	-0.051806	4.815561
248.581868	7999.980150	12.679386	-0.051796	4.815549
248.544032	8000.004114	12.684391	-0.051789	4.815556
248.506237	7999.971477	12.689395	-0.051783	4.815547
248.528302	8000.007098	12.694400	-0.051787	4.815557
248.479217	7999.989228	12.699405	-0.051778	4.815552
248.258732	7999.943998	12.704410	-0.051737	4.815540
248.510970	7999.988715	12.709415	-0.051784	4.815552
248.298300	7999.986331	12.714419	-0.051745	4.815552
248.344186	7999.960399	12.719424	-0.051754	4.815544
248.654311	7999.978294	12.724429	-0.051812	4.815548
248.614596	7999.970189	12.729434	-0.051804	4.815546
248.594982	7999.975227	12.734439	-0.051801	4.815547
248.567210	7999.960908	12.739443	-0.051796	4.815543
248.475621	7999.960500	12.744448	-0.051779	4.815543
248.809410	7999.999073	12.749453	-0.051842	4.815553
248.292602	7999.959686	12.754458	-0.051746	4.815544
248.553347	8000.029105	12.759463	-0.051794	4.815563
248.629246	7999.990848	12.764467	-0.051809	4.815552
248.611312	7999.949991	12.769472	-0.051806	4.815540
248.688203	7999.987575	12.774477	-0.051820	4.815550
248.655424	8000.026573	12.779482	-0.051814	4.815562
248.749216	8000.018511	12.784487	-0.051832	4.815559
248.387489	7999.975247	12.789491	-0.051765	4.815548
248.612632	8000.006706	12.794496	-0.051807	4.815556
248.660456	8000.018185	12.799501	-0.051816	4.815559
248.541301	7999.997035	12.804506	-0.051794	4.815554
248.743990	8000.021721	12.809511	-0.051832	4.815560
248.724188	8000.012873	12.814515	-0.051828	4.815557
248.583710	8000.028753	12.819520	-0.051803	4.815563
248.578960	8000.008403	12.824525	-0.051802	4.815557
248.599199	7999.982053	12.829530	-0.051806	4.815549
248.660873	8000.025796	12.834535	-0.051818	4.815562
248.480141	8000.022865	12.839539	-0.051784	4.815562
248.570928	8000.035045	12.844544	-0.051801	4.815565
248.677152	8000.030389	12.849549	-0.051821	4.815563
248.514473	8000.004257	12.854554	-0.051791	4.815556
248.663278	8000.026995	12.859559	-0.051819	4.815562
248.543742	7999.995160	12.864563	-0.051797	4.815553
248.640438	8000.003164	12.869568	-0.051815	4.815555
248.690043	8000.037099	12.874573	-0.051825	4.815565
248.502541	7999.992407	12.879578	-0.051790	4.815552
248.589215	8000.026946	12.884583	-0.051806	4.815562
248.422737	7999.993277	12.889587	-0.051775	4.815553
248.547430	7999.973971	12.894592	-0.051799	4.815547
248.730467	8000.029307	12.899597	-0.051833	4.815562
248.768965	7999.958400	12.904602	-0.051841	4.815541
248.745721	8000.012506	12.909607	-0.051836	4.815557
248.749366	8000.011516	12.914611	-0.051837	4.815557
248.686531	8000.022256	12.919616	-0.051826	4.815560
248.808929	8000.022136	12.924621	-0.051849	4.815560
248.669296	8000.013468	12.929626	-0.051823	4.815558
248.681586	8000.020094	12.934631	-0.051826	4.815560
248.411623	7999.986872	12.939635	-0.051775	4.815551
248.594773	7999.980268	12.944640	-0.051810	4.815548
248.735536	8000.010351	12.949645	-0.051836	4.815557
248.568972	7999.978815	12.954650	-0.051805	4.815548
248.637297	7999.993832	12.959655	-0.051818	4.815552
248.449345	7999.965152	12.964659	-0.051784	4.815545
248.627304	7999.981958	12.969664	-0.051817	4.815549
248.825202	8000.012974	12.974669	-0.051854	4.815557
248.490590	7999.947725	12.979674	-0.051792	4.815539
248.520484	7999.999493	12.984679	-0.051798	4.815554
248.658481	7999.996424	12.989683	-0.051824	4.815553
248.763467	8000.001360	12.994688	-0.051843	4.815554
248.883096	7999.999060	12.999693	-0.051866	4.815552
248.781115	7999.951491	13.004698	-0.051847	4.815539
248.879136	8000.030003	13.009703	-0.051866	4.815562
248.625356	7999.954325	13.014707	-0.051818	4.815541
248.762833	8000.009986	13.019712	-0.051844	4.815556
248.770456	8000.017604	13.024717	-0.051846	4.815558
248.664280	7999.963559	13.029722	-0.051826	4.815543
248.752518	7999.947930	13.034727	-0.051843	4.815538
248.601190	7999.957227	13.039731	-0.051815	4.815542
248.660080	7999.973158	13.044736	-0.051826	4.815546
248.644272	8000.006025	13.049741	-0.051823	4.815556
248.505896	7999.967474	13.054746	-0.051798	4.815545
248.704445	8000.021995	13.059751	-0.051835	4.815560
248.694079	7999.982330	13.064755	-0.051833	4.815548
248.698255	7999.986688	13.069760	-0.051834	4.815550
248.702963	8000.003871	13.074765	-0.051835	4.815555
248.642331	7999.968725	13.079770	-0.051824	4.815545
248.587950	7999.996691	13.084775	-0.051814	4.815553
248.399756	7999.977618	13.089779	-0.051780	4.815548
248.771949	8000.009342	13.094784	-0.051849	4.815556
249.038139	8000.027590	13.099789	-0.051899	4.815560
248.554593	8000.028259	13.104794	-0.051809	4.815562
248.586138	8000.035200	13.109799	-0.051815	4.815564
248.677175	7999.998257	13.114803	-0.051832	4.815553
248.510357	7999.987009	13.119808	-0.051801	4.815551
248.607974	7999.993961	13.124813	-0.051820	4.815552
248.351114	7999.974835	13.129818	-0.051772	4.815548
248.591047	8000.009741	13.134823	-0.051817	4.815557
248.534453	7999.966117	13.139827	-0.051807	4.815544
248.650090	7999.989382	13.144832	-0.051829	4.815551
248.693902	8000.024290	13.149837	-0.051837	4.815561
248.526725	7999.980997	13.154842	-0.051806	4.815549
248.810129	8000.005933	13.159847	-0.051859	4.815555
248.646249	8000.016092	13.164851	-0.051829	4.815558
248.798314	8000.013253	13.169856	-0.051857	4.815557
248.779374	8000.042865	13.174861	-0.051854	4.815566
248.759471	7999.995568	13.179866	-0.051850	4.815552
248.663287	8000.050618	13.184871	-0.051833	4.815568
248.630432	8000.006314	13.189875	-0.051827	4.815556
248.626447	8000.022287	13.194880	-0.051826	4.815560
248.898785	8000.027819	13.199885	-0.051877	4.815561
248.619167	7999.998709	13.204890	-0.051825	4.815553
248.468849	7999.988799	13.209895	-0.051797	4.815551
248.602864	7999.985665	13.214899	-0.051823	4.815550
248.590656	7999.978008	13.219904	-0.051821	4.815547
248.682136	8000.061753	13.224909	-0.051838	4.815572
248.607598	7999.972981	13.229914	-0.051824	4.815546
248.924774	8000.004876	13.234919	-0.051883	4.815554
248.586857	7999.985495	13.239923	-0.051821	4.815550
248.668785	7999.983647	13.244928	-0.051836	4.815549
248.714607	7999.998297	13.249933	-0.051845	4.815553
248.447530	7999.971529	13.254938	-0.051795	4.815546
248.712107	8000.031400	13.259943	-0.051845	4.815562
248.746679	8000.004215	13.264947	-0.051852	4.815554
248.702032	8000.028068	13.269952	-0.051843	4.815562
248.892194	8000.016239	13.274957	-0.051879	4.815557
248.571541	7999.989664	13.279962	-0.051820	4.815551
248.642354	7999.989770	13.284967	-0.051833	4.815551
248.568812	7999.983249	13.289971	-0.051819	4.815549
248.618668	8000.012916	13.294976	-0.051829	4.815557
248.452876	8000.008092	13.299981	-0.051798	4.815557
248.390661	7999.968649	13.304986	-0.051787	4.815546
248.422677	7999.975597	13.309991	-0.051793	4.815547
248.452841	7999.980380	13.314995	-0.051799	4.815549
248.567242	7999.997217	13.320000	-0.051820	4.815553
248.527285	8000.013671	13.325005	-0.051813	4.815558
248.476200	7999.982952	13.330010	-0.051804	4.815549
248.804282	8000.050268	13.335015	-0.051865	4.815567
248.885121	8000.007819	13.340019	-0.051880	4.815555
248.651464	8000.006159	13.345024	-0.051837	4.815555
248.608662	8000.026838	13.350029	-0.051829	4.815562
248.558985	7999.975852	13.355034	-0.051820	4.815547
248.721487	8000.022309	13.360039	-0.051851	4.815560
248.536938	8000.002228	13.365043	-0.051817	4.815555
248.633241	7999.965371	13.370048	-0.051835	4.815543
248.611853	8000.005623	13.375053	-0.051831	4.815555
248.634745	7999.969704	13.380058	-0.051835	4.815545
248.764479	8000.014559	13.385063	-0.051860	4.815557
248.668770	7999.978840	13.390067	-0.051842	4.815547
248.575842	8000.016857	13.395072	-0.051825	4.815559
248.882794	8000.035769	13.400077	-0.051883	4.815563
248.847540	8000.003173	13.405082	-0.051876	4.815553
248.678597	8000.022861	13.410087	-0.051845	4.815560
248.847955	8000.011760	13.415091	-0.051877	4.815556
248.972794	7999.988185	13.420096	-0.051900	4.815548
248.820366	8000.012415	13.425101	-0.051872	4.815556
248.581802	7999.982908	13.430106	-0.051828	4.815549
248.769498	8000.031913	13.435111	-0.051863	4.815562
248.819399	8000.011386	13.440115	-0.051872	4.815556
248.564627	8000.009382	13.445120	-0.051825	4.815557
248.743772	8000.039024	13.450125	-0.051859	4.815564
248.527483	8000.007744	13.455130	-0.051819	4.815556
248.558841	8000.038177	13.460135	-0.051825	4.815565
248.772535	7999.994693	13.465139	-0.051865	4.815551
248.552733	8000.009279	13.470144	-0.051824	4.815557
248.680139	8000.060504	13.475149	-0.051848	4.815571
248.646318	8000.000164	13.480154	-0.051842	4.815553
248.706683	7999.991556	13.485159	-0.051853	4.815551
248.845343	7999.993838	13.490163	-0.051879	4.815551
248.741539	7999.980414	13.495168	-0.051860	4.815547
248.921960	8000.019689	13.500173	-0.051894	4.815558
248.873795	8000.008241	13.505178	-0.051885	4.815555
248.852160	8000.014314	13.510183	-0.051881	4.815557
248.575068	7999.967091	13.515187	-0.051830	4.815544
248.857736	8000.008034	13.520192	-0.051883	4.815555
248.759980	8000.018205	13.525197	-0.051865	4.815558
248.601373	7999.966507	13.530202	-0.051836	4.815544
248.680974	7999.993456	13.535207	-0.051851	4.815551
248.920016	7999.976017	13.540211	-0.051895	4.815545
248.797688	8000.000738	13.545216	-0.051873	4.815553
248.918373	8000.033698	13.550221	-0.051895	4.815562
248.973105	7999.987619	13.555226	-0.051906	4.815548
249.037770	8000.045296	13.560231	-0.051918	4.815565
248.736903	8000.016907	13.565235	-0.051862	4.815558
248.769540	8000.011050	13.570240	-0.051869	4.815556
249.069452	8000.020237	13.575245	-0.051925	4.815557
248.759053	8000.013052	13.580250	-0.051867	4.815557
248.973062	8000.036856	13.585255	-0.051907	4.815562
249.099772	8000.025059	13.590259	-0.051931	4.815558
248.941281	8000.015014	13.595264	-0.051902	4.815556
248.831471	8000.033531	13.600269	-0.051881	4.815562
248.931131	8000.010613	13.605274	-0.051900	4.815555
249.098390	8000.045402	13.610279	-0.051932	4.815564
248.851159	8000.014684	13.615283	-0.051886	4.815557
248.925423	8000.009507	13.620288	-0.051900	4.815555
249.038350	8000.028457	13.625293	-0.051921	4.815560
248.752037	7999.988558	13.630298	-0.051868	4.815549
248.957491	7999.994066	13.635303	-0.051906	4.815550
248.963239	8000.005926	13.640307	-0.051908	4.815553
248.748462	8000.021662	13.645312	-0.051868	4.815559
248.832651	8000.025191	13.650317	-0.051884	4.815560
248.935492	7999.984169	13.655322	-0.051903	4.815547
249.038023	8000.031784	13.660327	-0.051922	4.815561
249.033382	8000.010367	13.665331	-0.051922	4.815554
248.884587	7999.962034	13.670336	-0.051894	4.815541
248.915249	8000.026631	13.675341	-0.051900	4.815560
248.901802	7999.968759	13.680346	-0.051898	4.815543
248.869385	8000.031259	13.685351	-0.051892	4.815561
248.951680	8000.036893	13.690355	-0.051908	4.815562
248.863748	8000.047223	13.695360	-0.051891	4.815566
248.957042	8000.046629	13.700365	-0.051909	4.815565
248.937394	8000.031375	13.705370	-0.051906	4.815561
249.013245	8000.014476	13.710375	-0.051920	4.815556
248.618556	7999.995236	13.715379	-0.051847	4.815552
248.804104	7999.984399	13.720384	-0.051881	4.815548
249.026710	8000.022227	13.725389	-0.051923	4.815558
248.882219	7999.979303	13.730394	-0.051896	4.815546
249.013270	8000.007093	13.735399	-0.051921	4.815553
248.875856	8000.000596	13.740403	-0.051896	4.815552
248.906544	8000.012863	13.745408	-0.051901	4.815556
248.950195	8000.033885	13.750413	-0.051910	4.815562
248.887464	7999.999772	13.755418	-0.051898	4.815552
248.786801	8000.054750	13.760423	-0.051880	4.815568
248.774301	8000.010777	13.765427	-0.051878	4.815556
248.709636	8000.005468	13.770432	-0.051866	4.815554
248.897624	8000.030983	13.775437	-0.051901	4.815561
248.927394	8000.020808	13.780442	-0.051907	4.815558
248.836312	8000.040699	13.785447	-0.051890	4.815564
248.705656	8000.004409	13.790451	-0.051866	4.815554
248.730214	7999.971721	13.795456	-0.051871	4.815544
248.804081	8000.027412	13.800461	-0.051885	4.815560
248.783475	8000.023890	13.805466	-0.051881	4.815559
249.100326	8000.036557	13.810471	-0.051940	4.815562
249.036195	8000.005625	13.815475	-0.051929	4.815553
248.794103	8000.033731	13.820480	-0.051884	4.815562
248.946022	8000.050113	13.825485	-0.051912	4.815566
248.747906	7999.998838	13.830490	-0.051875	4.815552
248.860904	8000.027400	13.835495	-0.051897	4.815560
248.965901	8000.044085	13.840499	-0.051917	4.815564
249.102479	8000.012158	13.845504	-0.051942	4.815554
248.970152	8000.042055	13.850509	-0.051918	4.815564
249.005210	8000.018082	13.855514	-0.051924	4.815557
249.038285	8000.036796	13.860519	-0.051931	4.815562
249.124813	8000.023276	13.865523	-0.051947	4.815557
249.004506	8000.002106	13.870528	-0.051925	4.815552
248.921495	8000.013585	13.875533	-0.051910	4.815556
248.804054	8000.004210	13.880538	-0.051888	4.815553
248.923893	8000.016865	13.885543	-0.051911	4.815557
249.013172	7999.995913	13.890547	-0.051927	4.815550
249.000683	8000.016020	13.895552	-0.051925	4.815556
249.096062	8000.048567	13.900557	-0.051943	4.815565
249.162998	8000.033658	13.905562	-0.051956	4.815560
248.968461	8000.052928	13.910567	-0.051920	4.815567
248.832173	8000.009070	13.915571	-0.051895	4.815555
248.775105	8000.003885	13.920576	-0.051884	4.815553
249.095301	8000.041170	13.925581	-0.051944	4.815563
248.898596	7999.976034	13.930586	-0.051908	4.815545
248.890366	8000.006890	13.935591	-0.051906	4.815554
248.694406	7999.983418	13.940595	-0.051870	4.815548
248.752252	7999.960885	13.945600	-0.051881	4.815541
248.879718	8000.017451	13.950605	-0.051905	4.815557
248.787299	8000.014893	13.955610	-0.051888	4.815557
248.829802	8000.049780	13.960615	-0.051896	4.815567
249.048302	8000.010647	13.965619	-0.051937	4.815554
248.901023	7999.985833	13.970624	-0.051910	4.815547
249.043200	8000.053319	13.975629	-0.051937	4.815567
249.066470	8000.006727	13.980634	-0.051941	4.815553
249.078341	8000.028298	13.985639	-0.051944	4.815559
248.992318	8000.009825	13.990643	-0.051928	4.815554
248.912267	7999.991448	13.995648	-0.051913	4.815549
248.980151	8000.012867	14.000653	-0.051926	4.815555
248.820488	8000.000667	14.005658	-0.051896	4.815552
249.071637	8000.049641	14.010663	-0.051943	4.815565
248.947052	8000.023061	14.015667	-0.051920	4.815558
248.833949	8000.002010	14.020672	-0.051899	4.815552
249.013251	8000.039131	14.025677	-0.051933	4.815562
249.130014	7999.987656	14.030682	-0.051955	4.815547
248.761289	8000.005150	14.035687	-0.051887	4.815554
248.879983	8000.023126	14.040691	-0.051909	4.815558
248.951650	8000.041402	14.045696	-0.051922	4.815563
249.094187	8000.051224	14.050701	-0.051949	4.815566
249.004600	7999.995313	14.055706	-0.051933	4.815550
248.920808	8000.043090	14.060711	-0.051917	4.815564
249.111783	8000.016323	14.065715	-0.051953	4.815555
248.975450	8000.022659	14.070720	-0.051928	4.815558
249.152226	8000.055468	14.075725	-0.051961	4.815567
249.022563	7999.982882	14.080730	-0.051937	4.815546
249.052906	8000.026115	14.085735	-0.051943	4.815558
249.184736	8000.033626	14.090739	-0.051968	4.815560
249.147128	8000.029826	14.095744	-0.051961	4.815559
249.084061	8000.024543	14.100749	-0.051949	4.815558
248.893130	7999.963773	14.105754	-0.051914	4.815541
249.018819	7999.974387	14.110759	-0.051938	4.815543
248.886644	7999.982928	14.115763	-0.051913	4.815547
248.949902	7999.993591	14.120768	-0.051925	4.815549
248.923514	8000.040169	14.125773	-0.051921	4.815563
248.994223	8000.010371	14.130778	-0.051934	4.815554
249.063487	8000.041424	14.135783	-0.051947	4.815563
248.961342	8000.063270	14.140787	-0.051928	4.815570
249.248720	8000.038077	14.145792	-0.051982	4.815561
249.372991	8000.057213	14.150797	-0.052005	4.815566
249.143614	8000.044942	14.155802	-0.051963	4.815563
248.888958	8000.024782	14.160807	-0.051916	4.815559
249.095969	8000.019637	14.165811	-0.051954	4.815556
248.879837	7999.965931	14.170816	-0.051914	4.815542
249.127001	8000.030860	14.175821	-0.051961	4.815559
249.130345	7999.778890	14.180826	-0.051961	4.815486

248.924283	7996.443837	14.185831	-0.051921	4.814512
248.946828	7990.758383	14.190835	-0.051922	4.812849
248.878080	7983.955250	14.195840	-0.051905	4.810859
248.834299	7976.680773	14.200845	-0.051892	4.808730
248.699340	7969.033963	14.205850	-0.051862	4.806491
248.823420	7961.225351	14.210855	-0.051880	4.804203
248.702516	7953.417763	14.215859	-0.051853	4.801916
248.709589	7945.326346	14.220864	-0.051849	4.799543
248.782164	7937.480346	14.225869	-0.051858	4.797241
248.936589	7929.370255	14.230874	-0.051881	4.794860
249.001533	7921.413775	14.235879	-0.051888	4.792523
248.755088	7913.366430	14.240883	-0.051838	4.790159
248.549044	7905.385311	14.245888	-0.051794	4.787814
248.770302	7897.402430	14.250893	-0.051830	4.785465
248.615550	7889.415077	14.255898	-0.051797	4.783116
248.653362	7881.403561	14.260903	-0.051799	4.780757
248.632166	7873.454554	14.265907	-0.051790	4.778416
248.542432	7865.386756	14.270912	-0.051768	4.776039
248.402702	7857.374248	14.275917	-0.051737	4.773677
248.371480	7849.348097	14.280922	-0.051726	4.771310
248.493043	7841.360642	14.285927	-0.051744	4.768952
248.418912	7833.430720	14.290931	-0.051725	4.766611
248.416716	7825.322816	14.295936	-0.051719	4.764216
248.366456	7817.466592	14.300941	-0.051705	4.761894
248.187243	7809.357284	14.305946	-0.051667	4.759496
248.377357	7801.454727	14.310951	-0.051697	4.757158
248.315486	7793.412896	14.315955	-0.051681	4.754777
248.193199	7785.266953	14.320960	-0.051653	4.752365
248.247952	7777.310424	14.325965	-0.051658	4.750008
248.207641	7769.298905	14.330970	-0.051645	4.747633
248.220247	7761.318285	14.335975	-0.051643	4.745266
248.083642	7753.363244	14.340979	-0.051612	4.742905
247.808861	7745.327769	14.345984	-0.051556	4.740520
247.996359	7737.401930	14.350989	-0.051586	4.738166
247.830496	7729.310580	14.355994	-0.051550	4.735761
247.906338	7721.317049	14.360999	-0.051559	4.733384
247.962320	7713.293753	14.366003	-0.051565	4.730997
247.943412	7705.267513	14.371008	-0.051556	4.728608
247.829050	7697.319948	14.376013	-0.051530	4.726242
247.612259	7689.250854	14.381018	-0.051485	4.723838
247.622158	7681.325071	14.386023	-0.051481	4.721475
247.577075	7673.329541	14.391027	-0.051468	4.719091
247.657898	7665.334930	14.396032	-0.051478	4.716705
247.457951	7657.303405	14.401037	-0.051436	4.714307
247.661398	7649.296976	14.406042	-0.051469	4.711915
247.679855	7641.238821	14.411047	-0.051467	4.709507
247.716530	7633.342544	14.416051	-0.051469	4.707146
247.545671	7625.264052	14.421056	-0.051432	4.704729
247.419578	7617.329831	14.426061	-0.051404	4.702355
247.426799	7609.278648	14.431066	-0.051400	4.699944
247.176498	7601.374679	14.436071	-0.051348	4.697576
247.162862	7593.294128	14.441075	-0.051341	4.695154
246.925469	7585.257980	14.446080	-0.051292	4.692744
247.196201	7577.279080	14.451085	-0.051337	4.690349
247.148887	7569.284609	14.456090	-0.051323	4.687949
247.301536	7561.277738	14.461095	-0.051347	4.685543
246.986182	7553.322195	14.466099	-0.051283	4.683153
246.986102	7545.238624	14.471104	-0.051278	4.680722
246.969167	7537.284701	14.476109	-0.051270	4.678329
247.035068	7529.302091	14.481114	-0.051277	4.675926
247.135216	7521.250149	14.486119	-0.051291	4.673501
247.156796	7513.153316	14.491123	-0.051290	4.671061
247.030148	7505.190512	14.496128	-0.051261	4.668660
246.980658	7497.241493	14.501133	-0.051247	4.666263
246.906470	7489.193070	14.506138	-0.051228	4.663834
246.712018	7481.231115	14.511143	-0.051187	4.661430
246.761331	7473.219467	14.516147	-0.051191	4.659009
246.506897	7465.231596	14.521152	-0.051139	4.656595
246.572660	7457.228353	14.526157	-0.051146	4.654175
246.452035	7449.228699	14.531162	-0.051118	4.651754
246.456594	7441.211963	14.536167	-0.051114	4.649327
246.359102	7433.272314	14.541171	-0.051091	4.646922
246.250329	7425.157594	14.546176	-0.051066	4.644463
246.527054	7417.270414	14.551181	-0.051112	4.642071
246.626164	7409.230462	14.556186	-0.051126	4.639632
246.337274	7401.251579	14.561191	-0.051067	4.637210
246.456191	7393.219072	14.566195	-0.051084	4.634771
246.473950	7385.165958	14.571200	-0.051082	4.632324
246.536445	7377.175675	14.576205	-0.051089	4.629894
246.266135	7369.179983	14.581210	-0.051034	4.627462
246.288451	7361.149888	14.586215	-0.051033	4.625019
246.142288	7353.245900	14.591219	-0.051001	4.622612
246.087661	7345.230371	14.596224	-0.050986	4.620170
246.138092	7337.221187	14.601229	-0.050990	4.617728
245.991038	7329.175275	14.606234	-0.050957	4.615274
245.723234	7321.167473	14.611239	-0.050903	4.612831
245.939806	7313.138324	14.616243	-0.050938	4.610379
245.851036	7305.154390	14.621248	-0.050916	4.607941
245.918919	7297.159300	14.626253	-0.050924	4.605497
245.861773	7289.219577	14.631258	-0.050908	4.603069
245.981538	7281.199214	14.636263	-0.050926	4.600615
245.968689	7273.215887	14.641267	-0.050918	4.598171
245.512908	7265.141675	14.646272	-0.050828	4.595698
245.619388	7257.144394	14.651277	-0.050843	4.593247
245.545094	7249.081447	14.656282	-0.050824	4.590775
245.525564	7241.135696	14.661287	-0.050816	4.588337
245.362555	7233.149763	14.666291	-0.050780	4.585886
245.319849	7225.103854	14.671296	-0.050767	4.583415
245.536421	7217.134760	14.676301	-0.050803	4.580966
245.155820	7209.115699	14.681306	-0.050727	4.578500
245.304824	7201.124885	14.686311	-0.050750	4.576042
245.269646	7193.151073	14.691315	-0.050738	4.573588
245.093444	7185.079675	14.696320	-0.050700	4.571102
245.154449	7177.133450	14.701325	-0.050707	4.568654
245.186334	7169.123745	14.706330	-0.050708	4.566185
245.090897	7161.120899	14.711335	-0.050685	4.563716
245.079272	7153.169612	14.716339	-0.050678	4.561263
245.209572	7145.110808	14.721344	-0.050697	4.558774
245.134825	7137.199741	14.726349	-0.050678	4.556330
244.884695	7129.127190	14.731354	-0.050626	4.553834
244.914737	7121.105212	14.736359	-0.050627	4.551353
245.074169	7113.061726	14.741363	-0.050652	4.548864
244.810070	7105.110530	14.746368	-0.050597	4.546402
244.990142	7097.090772	14.751373	-0.050626	4.543918
244.849431	7089.148666	14.756378	-0.050595	4.541456
244.610306	7081.158173	14.761383	-0.050545	4.538977
244.571998	7073.172931	14.766387	-0.050533	4.536499
244.693120	7065.116679	14.771392	-0.050551	4.533998
244.716536	7057.101637	14.776397	-0.050550	4.531509
244.418591	7049.097167	14.781402	-0.050490	4.529020
244.356743	7041.108641	14.786407	-0.050473	4.526536
244.623635	7033.119198	14.791411	-0.050518	4.524050
244.511384	7025.114751	14.796416	-0.050492	4.521558
244.626424	7017.142128	14.801421	-0.050508	4.519075
244.374082	7009.162645	14.806426	-0.050456	4.516587
244.641326	7001.102516	14.811431	-0.050501	4.514074
244.302327	6993.023648	14.816435	-0.050433	4.511552
244.232490	6984.997207	14.821440	-0.050415	4.509046
244.162871	6977.043204	14.826445	-0.050397	4.506562
244.087737	6969.040745	14.831450	-0.050378	4.504060
244.062622	6961.096222	14.836455	-0.050368	4.501576
244.171912	6953.097035	14.841459	-0.050384	4.499073
243.952664	6945.116256	14.846464	-0.050338	4.496574
243.835130	6937.079269	14.851469	-0.050311	4.494056
243.925777	6929.054800	14.856474	-0.050323	4.491541
244.166343	6921.034325	14.861479	-0.050362	4.489027
243.754275	6913.083461	14.866483	-0.050281	4.486531
243.714842	6905.037961	14.871488	-0.050268	4.484005
244.078160	6897.081270	14.876493	-0.050331	4.481507
243.854936	6889.068543	14.881498	-0.050284	4.478987
243.901533	6881.092254	14.886503	-0.050288	4.476479
243.724017	6873.074275	14.891507	-0.050250	4.473956
243.817448	6864.980554	14.896512	-0.050262	4.471408
243.778362	6857.030638	14.901517	-0.050250	4.468903
243.594754	6849.001709	14.906522	-0.050211	4.466372
243.670298	6841.025835	14.911527	-0.050220	4.463857
243.581855	6833.068258	14.916531	-0.050199	4.461346
243.648229	6824.987785	14.921536	-0.050206	4.458795
243.659709	6817.066717	14.926541	-0.050203	4.456292
243.479917	6809.033015	14.931546	-0.050165	4.453752
243.331036	6800.992727	14.936551	-0.050132	4.451209
243.456053	6793.013734	14.941555	-0.050150	4.448684
243.333164	6785.009943	14.946560	-0.050122	4.446150
243.178120	6777.016126	14.951565	-0.050088	4.443616
243.286061	6769.028316	14.956570	-0.050103	4.441085
243.257207	6761.051815	14.961575	-0.050093	4.438555
243.207019	6753.047723	14.966579	-0.050079	4.436014
243.149990	6744.947101	14.971584	-0.050063	4.433442
243.289372	6736.958434	14.976589	-0.050084	4.430904
243.181100	6728.947437	14.981594	-0.050059	4.428357
243.012249	6720.998896	14.986599	-0.050022	4.425828
242.958933	6712.967944	14.991603	-0.050007	4.423272
243.076397	6704.953801	14.996608	-0.050024	4.420720
243.012447	6697.019488	15.001613	-0.050007	4.418191
242.776185	6689.004300	15.006618	-0.049958	4.415635
242.935153	6680.980842	15.011623	-0.049983	4.413076
242.560760	6672.991917	15.016627	-0.049908	4.410524
242.630393	6664.990901	15.021632	-0.049916	4.407969
242.788904	6657.000879	15.026637	-0.049941	4.405417
242.579091	6648.981444	15.031642	-0.049897	4.402851
242.517944	6640.972115	15.036647	-0.049880	4.400288
242.642070	6633.030676	15.041651	-0.049898	4.397747
242.765199	6625.014878	15.046656	-0.049916	4.395180
242.652495	6616.990236	15.051661	-0.049890	4.392607
242.336617	6608.952461	15.056666	-0.049827	4.390028
242.571105	6600.954634	15.061671	-0.049865	4.387463
242.638662	6592.970191	15.066675	-0.049873	4.384900
242.158367	6585.006046	15.071680	-0.049778	4.382338
242.356006	6577.012141	15.076685	-0.049810	4.379770
242.255784	6569.051598	15.081690	-0.049787	4.377209
242.193530	6561.006806	15.086695	-0.049770	4.374620
242.099904	6552.995503	15.091699	-0.049747	4.372039
242.035350	6544.911903	15.096704	-0.049730	4.369434
242.224613	6537.013216	15.101709	-0.049761	4.366889
241.826817	6529.011379	15.106714	-0.049682	4.364305
242.057496	6521.038953	15.111719	-0.049720	4.361733
242.164390	6512.968246	15.116723	-0.049734	4.359127
241.990772	6505.034418	15.121728	-0.049697	4.356562
241.836772	6497.004564	15.126733	-0.049663	4.353965
241.861153	6488.840912	15.131738	-0.049663	4.351323
241.747302	6480.889417	15.136743	-0.049637	4.348748
241.854687	6472.925594	15.141747	-0.049652	4.346169
241.955708	6464.938672	15.146752	-0.049666	4.343581
241.830951	6456.974696	15.151757	-0.049637	4.340997
241.687700	6448.964938	15.156762	-0.049606	4.338397
241.963810	6440.953954	15.161767	-0.049652	4.335798
241.987487	6432.991547	15.166771	-0.049651	4.333211
241.398548	6424.922444	15.171776	-0.049537	4.330583
241.418363	6416.992846	15.176781	-0.049535	4.328004
241.423776	6408.971451	15.181786	-0.049531	4.325393
241.385367	6400.977926	15.186791	-0.049519	4.322789
241.445543	6392.976480	15.191795	-0.049526	4.320182
241.400780	6384.987022	15.196800	-0.049512	4.317576
241.518527	6376.951812	15.201805	-0.049529	4.314956
241.640227	6368.925176	15.206810	-0.049547	4.312336
241.539552	6360.877040	15.211815	-0.049523	4.309706
241.373781	6352.961429	15.216819	-0.049487	4.307117
241.259857	6344.918694	15.221824	-0.049461	4.304486
241.130527	6336.973800	15.226829	-0.049432	4.301884
241.117434	6328.932804	15.231834	-0.049424	4.299251
241.067328	6320.957653	15.236839	-0.049410	4.296637
241.130585	6312.929395	15.241843	-0.049417	4.294005
241.035182	6304.879519	15.246848	-0.049394	4.291364
241.165897	6296.859440	15.251853	-0.049413	4.288732
240.959009	6288.924916	15.256858	-0.049370	4.286124
241.045306	6280.915737	15.261863	-0.049381	4.283492
241.090804	6272.991254	15.266867	-0.049384	4.280886
240.949232	6264.928442	15.271872	-0.049353	4.278231
240.809348	6256.959746	15.276877	-0.049322	4.275606
240.864559	6248.880105	15.281882	-0.049327	4.272944
240.551259	6240.861540	15.286887	-0.049264	4.270297
240.612167	6232.928054	15.291891	-0.049270	4.267681
240.508921	6224.873322	15.296896	-0.049246	4.265021
240.531785	6216.910983	15.301901	-0.049245	4.262391
240.502666	6208.875646	15.306906	-0.049235	4.259734
240.339590	6200.923534	15.311911	-0.049199	4.257103
240.497080	6192.918586	15.316915	-0.049224	4.254455
240.160035	6184.887920	15.321920	-0.049156	4.251793
240.245400	6176.905315	15.326925	-0.049167	4.249148
240.116426	6168.918591	15.331930	-0.049138	4.246499
240.048043	6160.903219	15.336935	-0.049120	4.243839
240.244098	6152.935229	15.341939	-0.049152	4.241196
240.059535	6144.932275	15.346944	-0.049112	4.238535
240.142082	6136.961484	15.351949	-0.049123	4.235887
240.089563	6128.927312	15.356954	-0.049108	4.233214
239.923727	6120.865912	15.361959	-0.049072	4.230529
240.209571	6112.918279	15.366963	-0.049120	4.227885
240.272748	6104.912780	15.371968	-0.049127	4.225218
239.900216	6096.960839	15.376973	-0.049053	4.222563
239.808798	6088.940169	15.381978	-0.049031	4.219886
239.847938	6080.930984	15.386983	-0.049033	4.217212
239.719996	6072.963696	15.391987	-0.049004	4.214549
239.691281	6064.887379	15.396992	-0.048994	4.211849
239.869670	6056.921861	15.401997	-0.049022	4.209186
239.790453	6048.925454	15.407002	-0.049002	4.206509
239.501177	6040.944435	15.412007	-0.048943	4.203833
239.473418	6033.021902	15.417011	-0.048933	4.201177
239.408184	6024.967846	15.422016	-0.048916	4.198475
239.360288	6016.982629	15.427021	-0.048902	4.195795
239.483520	6008.877195	15.432026	-0.048920	4.193074
239.118082	6000.807506	15.437031	-0.048847	4.190359
239.265470	5992.881673	15.442035	-0.048869	4.187696
239.265402	5984.861722	15.447040	-0.048864	4.184997
239.558362	5976.917111	15.452045	-0.048914	4.182326
239.468596	5968.858476	15.457050	-0.048892	4.179610
239.285749	5960.956328	15.462055	-0.048853	4.176944
239.495807	5952.939855	15.467059	-0.048887	4.174242
239.263512	5944.884096	15.472064	-0.048839	4.171520
239.063774	5936.927777	15.477069	-0.048797	4.168831
239.038981	5928.913516	15.482074	-0.048787	4.166122
239.017631	5920.881299	15.487079	-0.048778	4.163405
238.928835	5912.942411	15.492083	-0.048757	4.160717
238.708552	5904.920134	15.497088	-0.048711	4.157998
239.007504	5896.902750	15.502093	-0.048761	4.155285
238.959292	5888.887831	15.507098	-0.048747	4.152566
238.863691	5880.887202	15.512103	-0.048724	4.149851
239.027027	5872.888270	15.517107	-0.048750	4.147137
238.905388	5864.864169	15.522112	-0.048722	4.144409
238.858222	5856.947411	15.527117	-0.048708	4.141717
238.635168	5848.886156	15.532122	-0.048662	4.138972
238.550099	5840.922569	15.537127	-0.048641	4.136260
238.633179	5832.889460	15.542131	-0.048652	4.133524
238.681302	5824.851010	15.547136	-0.048655	4.130785
238.586367	5816.877084	15.552141	-0.048633	4.128063
238.442250	5808.882837	15.557146	-0.048601	4.125333
238.575309	5800.896515	15.562151	-0.048621	4.122607
238.559908	5792.923674	15.567155	-0.048613	4.119882
238.478800	5784.913857	15.572160	-0.048593	4.117141
238.282229	5776.890943	15.577165	-0.048551	4.114393
238.079582	5768.890110	15.582170	-0.048508	4.111650
238.075658	5760.834362	15.587175	-0.048503	4.108889
238.143394	5752.895979	15.592179	-0.048510	4.106168
237.970986	5744.878348	15.597184	-0.048473	4.103414
238.349976	5736.927686	15.602189	-0.048539	4.100689
238.139900	5728.945883	15.607194	-0.048495	4.097944
237.944365	5720.948989	15.612199	-0.048453	4.095191
238.083460	5712.907313	15.617203	-0.048474	4.092426
238.073113	5704.867819	15.622208	-0.048467	4.089658
238.085220	5696.932532	15.627213	-0.048464	4.086924
238.001148	5688.908605	15.632218	-0.048444	4.084156
238.127783	5680.954140	15.637223	-0.048462	4.081414
238.050125	5672.968851	15.642227	-0.048443	4.078656
237.789763	5664.952984	15.647232	-0.048389	4.075883
237.803390	5656.957803	15.652237	-0.048387	4.073119
237.643924	5648.910120	15.657242	-0.048352	4.070332
237.498896	5640.921522	15.662247	-0.048320	4.067565
237.438461	5632.948477	15.667251	-0.048304	4.064802
237.629929	5624.966017	15.672256	-0.048335	4.062037
237.658446	5616.960570	15.677261	-0.048335	4.059260
237.446041	5608.970603	15.682266	-0.048290	4.056484
237.347896	5600.925732	15.687271	-0.048267	4.053688
237.497343	5592.912889	15.692275	-0.048290	4.050904
237.191168	5584.902259	15.697280	-0.048228	4.048113
237.357566	5576.919429	15.702285	-0.048254	4.045337
237.361010	5568.974030	15.707290	-0.048250	4.042569
237.238789	5560.936482	15.712295	-0.048222	4.039766
237.213538	5552.993460	15.717299	-0.048212	4.036995
237.088350	5544.927892	15.722304	-0.048184	4.034177
236.992576	5536.841729	15.727309	-0.048161	4.031351
236.955582	5528.848009	15.732314	-0.048149	4.028556
237.024742	5520.862360	15.737319	-0.048157	4.025764
236.799518	5512.912082	15.742323	-0.048110	4.022978
236.687583	5504.907182	15.747328	-0.048084	4.020172
237.079166	5496.936393	15.752333	-0.048152	4.017384
236.913752	5488.926337	15.757338	-0.048116	4.014572
236.772995	5480.900420	15.762343	-0.048085	4.011752
236.989564	5472.909504	15.767347	-0.048120	4.008949
236.807940	5464.927816	15.772352	-0.048082	4.006140
236.628682	5456.928634	15.777357	-0.048043	4.003323
236.397824	5448.956125	15.782362	-0.047995	4.000513
236.697533	5440.924371	15.787367	-0.048046	3.997689
236.752207	5432.945695	15.792371	-0.048051	3.994877
236.692927	5424.904430	15.797376	-0.048035	3.992040
236.616351	5416.887395	15.802381	-0.048016	3.989208
236.431931	5408.933215	15.807386	-0.047977	3.986395
236.330333	5400.894360	15.812391	-0.047953	3.983552
236.197776	5392.958018	15.817395	-0.047923	3.980742
236.167570	5384.948485	15.822400	-0.047912	3.977906
236.049775	5376.948813	15.827405	-0.047885	3.975070
236.175051	5368.910827	15.832410	-0.047904	3.972222
236.095318	5360.905018	15.837415	-0.047884	3.969381
235.945352	5352.987448	15.842419	-0.047851	3.966567
236.060108	5344.946050	15.847424	-0.047867	3.963712
236.168336	5336.980940	15.852429	-0.047882	3.960882
236.130886	5328.997822	15.857434	-0.047870	3.958041
235.907998	5321.001405	15.862439	-0.047824	3.955190
235.635946	5312.986972	15.867443	-0.047768	3.952330
235.687090	5304.939029	15.872448	-0.047773	3.949461
235.932867	5296.964330	15.877453	-0.047814	3.946619
235.833696	5288.972947	15.882458	-0.047790	3.943764
235.783514	5280.974496	15.887463	-0.047776	3.940905
235.899224	5273.019891	15.892467	-0.047792	3.938062
235.627471	5265.010076	15.897472	-0.047737	3.935191
235.432861	5257.003239	15.902477	-0.047695	3.932320
235.443166	5248.961565	15.907482	-0.047692	3.929438
235.526322	5240.989119	15.912487	-0.047703	3.926580
235.437462	5233.023332	15.917491	-0.047681	3.923720
235.270555	5225.005676	15.922496	-0.047645	3.920837
235.299143	5217.024827	15.927501	-0.047646	3.917969
235.419414	5208.972243	15.932506	-0.047663	3.915074
235.322556	5200.971410	15.937511	-0.047640	3.912192
235.409490	5192.989560	15.942515	-0.047651	3.909318
235.465491	5185.013419	15.947520	-0.047656	3.906444
235.333321	5176.996688	15.952525	-0.047627	3.903549
235.297135	5169.018990	15.957530	-0.047615	3.900668
235.066251	5161.016808	15.962535	-0.047567	3.897773
235.116738	5153.029191	15.967539	-0.047572	3.894885
235.169759	5144.961102	15.972544	-0.047576	3.891967
235.203818	5136.951762	15.977549	-0.047578	3.889067
234.881198	5129.028486	15.982554	-0.047513	3.886190
234.748407	5121.002137	15.987559	-0.047483	3.883276
234.930426	5113.009734	15.992563	-0.047512	3.880379
234.808393	5105.045580	15.997568	-0.047484	3.877484
234.703139	5097.003245	16.002573	-0.047459	3.874559
234.633444	5088.756636	16.007578	-0.047441	3.871557
234.686667	5080.840685	16.012583	-0.047446	3.868677
234.653513	5072.925041	16.017587	-0.047435	3.865792
234.543259	5064.903985	16.022592	-0.047410	3.862866
234.671134	5056.946982	16.027597	-0.047428	3.859965
234.394978	5049.019877	16.032602	-0.047372	3.857065
234.366927	5040.986075	16.037607	-0.047362	3.854129
234.650591	5032.994886	16.042611	-0.047410	3.851212
234.575759	5025.010830	16.047616	-0.047391	3.848289
234.409710	5016.987701	16.052621	-0.047355	3.845347
234.376589	5009.047631	16.057626	-0.047344	3.842436
234.417131	5001.034586	16.062631	-0.047346	3.839498
234.069541	4993.082724	16.067635	-0.047277	3.836571
234.105992	4985.048227	16.072640	-0.047278	3.833620
234.288029	4977.013331	16.077645	-0.047307	3.830670
234.151364	4969.038349	16.082650	-0.047277	3.827733
234.031676	4961.032985	16.087655	-0.047249	3.824783
234.312485	4953.064219	16.092659	-0.047297	3.821852
234.192584	4945.089835	16.097664	-0.047269	3.818909
234.133489	4937.070791	16.102669	-0.047253	3.815948
234.161686	4929.081668	16.107674	-0.047254	3.812997
234.048901	4921.050360	16.112679	-0.047228	3.810026
233.942436	4913.129608	16.117683	-0.047203	3.807094
233.827881	4905.079772	16.122688	-0.047176	3.804111
234.000901	4897.121322	16.127693	-0.047204	3.801166
233.784275	4889.132187	16.132698	-0.047158	3.798199
233.645706	4881.117026	16.137703	-0.047128	3.795221
233.478368	4873.095644	16.142707	-0.047091	3.792239
233.326567	4865.051180	16.147712	-0.047058	3.789245
233.484304	4857.072680	16.152717	-0.047082	3.786281
233.429705	4849.093808	16.157722	-0.047067	3.783309
233.427743	4841.083727	16.162727	-0.047062	3.780325
233.305007	4833.140828	16.167731	-0.047034	3.777361
233.358409	4825.076483	16.172736	-0.047039	3.774353
233.221657	4817.096106	16.177741	-0.047009	3.771369
233.267825	4809.077574	16.182746	-0.047012	3.768373
233.064864	4801.083957	16.187751	-0.046969	3.765379
233.242353	4793.128504	16.192755	-0.046997	3.762405
233.276878	4785.075604	16.197760	-0.046999	3.759389
233.253289	4777.174235	16.202765	-0.046989	3.756425
233.103377	4769.121429	16.207770	-0.046957	3.753400
233.231217	4761.092025	16.212775	-0.046975	3.750388
232.971046	4753.141329	16.217779	-0.046922	3.747394
232.773278	4745.101121	16.222784	-0.046880	3.744365
232.887751	4737.163184	16.227789	-0.046896	3.741379
232.994118	4729.130994	16.232794	-0.046911	3.738355
232.828213	4721.134006	16.237799	-0.046875	3.735336
232.769301	4713.145069	16.242803	-0.046859	3.732320
232.648642	4705.132658	16.247808	-0.046832	3.729291
232.648781	4697.181055	16.252813	-0.046827	3.726285
232.709471	4689.167665	16.257818	-0.046833	3.723255
232.729108	4681.176591	16.262823	-0.046832	3.720231
232.681137	4673.205413	16.267827	-0.046818	3.717209
232.492988	4665.186399	16.272832	-0.046778	3.714164
232.503688	4657.121745	16.277837	-0.046775	3.711103
232.480501	4649.105374	16.282842	-0.046765	3.708058
232.382758	4641.110299	16.287847	-0.046742	3.705016
232.250807	4633.210190	16.292851	-0.046713	3.702007
232.208572	4625.179578	16.297856	-0.046700	3.698948
232.229567	4617.249754	16.302861	-0.046699	3.695926
232.071867	4609.244062	16.307866	-0.046664	3.692869
232.083823	4601.194651	16.312871	-0.046662	3.689797
232.140078	4593.235601	16.317875	-0.046667	3.686757
232.155102	4585.185441	16.322880	-0.046665	3.683680
231.862853	4577.252958	16.327885	-0.046606	3.680637
231.977697	4569.276392	16.332890	-0.046622	3.677585
231.871867	4561.241377	16.337895	-0.046597	3.674502
231.921687	4553.219800	16.342899	-0.046601	3.671426
231.579373	4545.219929	16.347904	-0.046533	3.668345
231.792858	4537.212177	16.352909	-0.046567	3.665274
231.752746	4529.255794	16.357914	-0.046555	3.662212
231.740531	4521.233662	16.362919	-0.046548	3.659124
231.822944	4513.293688	16.367923	-0.046558	3.656067
231.550305	4505.259911	16.372928	-0.046502	3.652963
231.817872	4497.212298	16.377933	-0.046547	3.649864
231.833622	4489.231509	16.382938	-0.046545	3.646782
231.417708	4481.256492	16.387943	-0.046463	3.643688
231.387750	4473.311008	16.392947	-0.046452	3.640613
231.409430	4465.297762	16.397952	-0.046451	3.637511
231.454056	4457.292977	16.402957	-0.046454	3.634410
231.305086	4449.270669	16.407962	-0.046422	3.631294
231.145223	4441.261705	16.412967	-0.046387	3.628180
231.161144	4433.277108	16.417971	-0.046385	3.625078
231.084424	4425.285784	16.422976	-0.046366	3.621969
231.185530	4417.289652	16.427981	-0.046379	3.618859
231.292959	4409.298304	16.432986	-0.046394	3.615749
231.224589	4401.287009	16.437991	-0.046377	3.612624
231.020449	4393.308308	16.442995	-0.046334	3.609504
230.965414	4385.326793	16.448000	-0.046318	3.606385
230.893317	4377.339858	16.453005	-0.046300	3.603261
230.919215	4369.364046	16.458010	-0.046300	3.600141
230.850470	4361.392365	16.463015	-0.046282	3.597018
230.934771	4353.407085	16.468019	-0.046293	3.593891
230.818721	4345.365208	16.473024	-0.046266	3.590733
230.725998	4337.395541	16.478029	-0.046244	3.587601
230.678892	4329.371603	16.483034	-0.046230	3.584447
230.742166	4321.413379	16.488039	-0.046237	3.581318
230.443335	4313.422677	16.493043	-0.046176	3.578164
230.436126	4305.399636	16.498048	-0.046170	3.575003
230.548370	4297.402645	16.503053	-0.046186	3.571852
230.492988	4289.385447	16.508058	-0.046170	3.568686
230.298818	4281.410102	16.513063	-0.046129	3.565530
230.550638	4273.445283	16.518067	-0.046171	3.562388
230.421066	4265.412323	16.523072	-0.046142	3.559205
230.329251	4257.482286	16.528077	-0.046120	3.556061
230.263406	4249.415697	16.533082	-0.046103	3.552861
230.337491	4241.332601	16.538087	-0.046111	3.549656
230.188248	4233.403122	16.543091	-0.046079	3.546502
230.129287	4225.390789	16.548096	-0.046063	3.543315
230.115931	4217.432461	16.553101	-0.046055	3.540148
229.790180	4209.490712	16.558106	-0.045990	3.536976
229.775682	4201.439556	16.563111	-0.045982	3.533766
229.957139	4193.435628	16.568115	-0.046011	3.530578
229.858973	4185.426493	16.573120	-0.045987	3.527377
229.815590	4177.439243	16.578125	-0.045974	3.524183
229.830885	4169.506259	16.583130	-0.045972	3.521010
229.795721	4161.506356	16.588135	-0.045961	3.517805
229.730710	4153.508267	16.593139	-0.045944	3.514598
229.693004	4145.485854	16.598144	-0.045931	3.511378
229.927187	4137.470057	16.603149	-0.045970	3.508167
229.766328	4129.491266	16.608154	-0.045935	3.504955
229.503238	4121.551062	16.613159	-0.045881	3.501753
229.625775	4113.569681	16.618163	-0.045899	3.498543
229.618309	4105.545303	16.623168	-0.045893	3.495309
229.609789	4097.515290	16.628173	-0.045886	3.492070
229.376825	4089.538133	16.633178	-0.045838	3.488842
229.320537	4081.555377	16.638183	-0.045822	3.485614
229.431574	4073.618569	16.643187	-0.045838	3.482407
229.277530	4065.623609	16.648192	-0.045804	3.479165
229.449820	4057.656578	16.653197	-0.045831	3.475942
229.251750	4049.627744	16.658202	-0.045789	3.472679
228.941296	4041.574747	16.663207	-0.045727	3.469399
229.166126	4033.618952	16.668211	-0.045763	3.466173
229.117344	4025.602553	16.673216	-0.045749	3.462911
228.969875	4017.607766	16.678221	-0.045717	3.459651
228.991225	4009.688971	16.683226	-0.045716	3.456424
229.049400	4001.615493	16.688231	-0.045722	3.453133
229.042878	3993.635914	16.693235	-0.045715	3.449874
228.741565	3985.635781	16.698240	-0.045654	3.446594
229.010403	3977.659014	16.703245	-0.045699	3.443340
228.889271	3969.677130	16.708250	-0.045672	3.440068
228.766988	3961.702233	16.713255	-0.045644	3.436795
228.561062	3953.709872	16.718259	-0.045601	3.433509
228.587956	3945.659115	16.723264	-0.045601	3.430204
228.605922	3937.688957	16.728269	-0.045599	3.426928
228.602264	3929.706958	16.733274	-0.045593	3.423644
228.364071	3921.719357	16.738279	-0.045544	3.420346
228.617430	3913.748961	16.743283	-0.045586	3.417069
228.541940	3905.721046	16.748288	-0.045567	3.413754
228.334066	3897.716480	16.753293	-0.045523	3.410440
228.380636	3889.732608	16.758298	-0.045527	3.407141
228.412065	3881.718506	16.763303	-0.045528	3.403825
228.366644	3873.812025	16.768307	-0.045515	3.400548
228.323968	3865.809862	16.773312	-0.045502	3.397229
228.264758	3857.786108	16.778317	-0.045486	3.393896
228.292829	3849.705848	16.783322	-0.045486	3.390540
228.266612	3841.716937	16.788327	-0.045476	3.387217
228.278251	3833.788155	16.793331	-0.045473	3.383917
227.826342	3825.812746	16.798336	-0.045384	3.380577
227.899489	3817.840529	16.803341	-0.045393	3.377254
227.915335	3809.847369	16.808346	-0.045391	3.373918
227.888898	3801.801509	16.813351	-0.045381	3.370554
227.962733	3793.864773	16.818355	-0.045389	3.367236
227.901342	3785.843090	16.823360	-0.045373	3.363875
227.868946	3777.875354	16.828365	-0.045362	3.360534
227.603426	3769.933383	16.833370	-0.045308	3.357192
227.567400	3761.872688	16.838375	-0.045296	3.353805
227.685741	3753.862480	16.843379	-0.045313	3.350441
227.641256	3745.875847	16.848384	-0.045300	3.347078
227.718727	3737.873349	16.853389	-0.045309	3.343709
227.605475	3729.915451	16.858394	-0.045283	3.340349
227.335799	3721.926034	16.863399	-0.045228	3.336966
227.574807	3713.924036	16.868403	-0.045267	3.333594
227.412929	3705.906854	16.873408	-0.045232	3.330196
227.301055	3697.944393	16.878413	-0.045206	3.326820
227.229143	3689.971833	16.883418	-0.045188	3.323438
227.193100	3681.991027	16.888423	-0.045176	3.320051
227.379354	3674.031076	16.893427	-0.045206	3.316677
227.120011	3666.001164	16.898432	-0.045152	3.313253
227.139407	3657.966681	16.903437	-0.045151	3.309834
227.195007	3650.000258	16.908442	-0.045156	3.306442
227.091996	3641.998323	16.913447	-0.045132	3.303025
227.138473	3634.033762	16.918451	-0.045136	3.299627
227.039820	3626.058981	16.923456	-0.045113	3.296214
227.047432	3618.075684	16.928461	-0.045109	3.292799
226.862922	3610.057464	16.933466	-0.045070	3.289358
226.732764	3602.101785	16.938471	-0.045040	3.285942
226.913146	3594.090787	16.943475	-0.045069	3.282511
226.789020	3586.118533	16.948480	-0.045041	3.279082
226.832842	3578.126398	16.953485	-0.045044	3.275646
226.716466	3570.118045	16.958490	-0.045017	3.272194
226.579745	3562.099059	16.963495	-0.044987	3.268732
226.817635	3554.124615	16.968499	-0.045026	3.265301
226.697633	3546.134085	16.973504	-0.044999	3.261846
226.442269	3538.179641	16.978509	-0.044946	3.258396
226.513336	3530.187917	16.983514	-0.044955	3.254940
226.401881	3522.165989	16.988519	-0.044929	3.251460
226.564777	3514.165540	16.993523	-0.044954	3.247997
226.475297	3506.167402	16.998528	-0.044932	3.244520
226.307898	3498.238219	17.003533	-0.044896	3.241067
226.543506	3490.242176	17.008538	-0.044935	3.237597
226.329427	3482.236229	17.013543	-0.044890	3.234101
226.223424	3474.191053	17.018547	-0.044866	3.230589
226.167598	3466.210753	17.023552	-0.044850	3.227103
226.274150	3458.223203	17.028557	-0.044865	3.223616
226.131586	3450.264030	17.033562	-0.044834	3.220128
225.963936	3442.301662	17.038567	-0.044797	3.216634
225.939762	3434.305346	17.043571	-0.044788	3.213127
225.905858	3426.274619	17.048576	-0.044776	3.209601
225.802310	3418.306185	17.053581	-0.044752	3.206095
225.852772	3410.333354	17.058586	-0.044757	3.202590
225.734229	3402.352674	17.063591	-0.044730	3.199071
225.669728	3394.425950	17.068595	-0.044713	3.195574
225.540280	3386.364954	17.073600	-0.044683	3.192010
225.474651	3378.371194	17.078605	-0.044666	3.188476
225.542351	3370.368640	17.083610	-0.044674	3.184939
225.564087	3362.376533	17.088615	-0.044673	3.181401
225.615968	3354.402379	17.093619	-0.044678	3.177868
225.547855	3346.414872	17.098624	-0.044660	3.174320
225.575521	3338.413048	17.103629	-0.044660	3.170766
225.582149	3330.441159	17.108634	-0.044656	3.167220
225.183379	3322.485920	17.113639	-0.044577	3.163660
225.165949	3314.516133	17.118643	-0.044569	3.160107
225.107668	3306.526436	17.123648	-0.044553	3.156538
225.221030	3298.494170	17.128653	-0.044569	3.152954
225.139879	3290.489271	17.133658	-0.044549	3.149370
225.031995	3282.494750	17.138663	-0.044524	3.145785
225.183955	3274.520123	17.143667	-0.044547	3.142216
225.095426	3266.557241	17.148672	-0.044526	3.138638
224.782625	3258.590832	17.153677	-0.044462	3.135044
224.875642	3250.577764	17.158682	-0.044475	3.131443
224.793947	3242.578655	17.163687	-0.044455	3.127837
224.816400	3234.613797	17.168691	-0.044454	3.124246
224.737167	3226.681991	17.173696	-0.044434	3.120662
224.731681	3218.653295	17.178701	-0.044428	3.117033
224.874276	3210.659898	17.183706	-0.044450	3.113422
224.839972	3202.608632	17.188711	-0.044438	3.109773
224.799806	3194.675425	17.193715	-0.044426	3.106173
224.741363	3186.664628	17.198720	-0.044410	3.102533
224.455313	3178.727273	17.203725	-0.044352	3.098911
224.523307	3170.745253	17.208730	-0.044359	3.095281
224.448892	3162.717064	17.213735	-0.044340	3.091620
224.587493	3154.741905	17.218739	-0.044361	3.087988
224.464503	3146.736927	17.223744	-0.044333	3.084325
224.423732	3138.811655	17.228749	-0.044321	3.080699
224.369011	3130.837865	17.233754	-0.044306	3.077046
224.245761	3122.779804	17.238759	-0.044278	3.073346
224.204048	3114.749720	17.243763	-0.044265	3.069659
224.153328	3106.762819	17.248768	-0.044250	3.065986
224.238415	3098.800114	17.253773	-0.044261	3.062327
224.138256	3090.873989	17.258778	-0.044238	3.058672
224.124206	3082.859247	17.263783	-0.044230	3.054975
223.966738	3074.884504	17.268787	-0.044196	3.051285
223.839055	3066.895498	17.273792	-0.044167	3.047586
223.729638	3058.919766	17.278797	-0.044142	3.043889
223.696634	3050.961366	17.283802	-0.044130	3.040200
223.580779	3042.976172	17.288807	-0.044104	3.036489
223.968045	3034.951272	17.293811	-0.044171	3.032780
223.713018	3026.953134	17.298816	-0.044118	3.029048
223.473054	3019.007637	17.303821	-0.044069	3.025336
223.410834	3011.035398	17.308826	-0.044052	3.021616
223.483347	3003.034864	17.313831	-0.044061	3.017884
223.495481	2995.061861	17.318835	-0.044058	3.014158
223.411283	2987.051486	17.323840	-0.044037	3.010405
223.337508	2979.087337	17.328845	-0.044019	3.006670
223.446502	2971.097914	17.333850	-0.044034	3.002927
223.376733	2963.112021	17.338855	-0.044016	2.999172
223.391686	2955.157061	17.343859	-0.044014	2.995431
223.365214	2947.121015	17.348864	-0.044004	2.991645
223.332214	2939.116361	17.353869	-0.043993	2.987869
223.261571	2931.155583	17.358874	-0.043974	2.984107
223.060406	2923.202940	17.363879	-0.043932	2.980338
223.190101	2915.227146	17.368883	-0.043951	2.976569
223.116737	2907.227787	17.373888	-0.043933	2.972774
222.940884	2899.236505	17.378893	-0.043895	2.968973
222.906660	2891.252178	17.383898	-0.043883	2.965178
222.735256	2883.299391	17.388903	-0.043847	2.961386
222.792748	2875.338792	17.393907	-0.043852	2.957596
222.740452	2867.330868	17.398912	-0.043838	2.953774
222.931391	2859.305102	17.403917	-0.043868	2.949951
222.852338	2851.344303	17.408922	-0.043848	2.946140
222.741320	2843.354309	17.413927	-0.043823	2.942308
222.656429	2835.414892	17.418931	-0.043802	2.938497
222.407323	2827.431550	17.423936	-0.043751	2.934652
222.533205	2819.407550	17.428941	-0.043769	2.930801
222.661019	2811.437894	17.433946	-0.043788	2.926971
222.451102	2803.470876	17.438951	-0.043744	2.923120
222.311980	2795.531276	17.443955	-0.043713	2.919281
222.275370	2787.547687	17.448960	-0.043701	2.915421
222.227593	2779.475984	17.453965	-0.043687	2.911513
222.139802	2771.474283	17.458970	-0.043666	2.907631
222.153954	2763.486211	17.463975	-0.043663	2.903756
222.144567	2755.546716	17.468979	-0.043657	2.899898
221.853858	2747.593147	17.473984	-0.043598	2.896013
221.934582	2739.589354	17.478989	-0.043608	2.892118
222.066528	2731.591887	17.483994	-0.043627	2.888224
221.881243	2723.623200	17.488999	-0.043588	2.884322
221.997255	2715.671985	17.494003	-0.043604	2.880439
221.792905	2707.730904	17.499008	-0.043561	2.876538
221.592155	2699.727149	17.504013	-0.043519	2.872602
221.720104	2691.733841	17.509018	-0.043538	2.868683
221.678835	2683.711389	17.514023	-0.043525	2.864735
221.851288	2675.757701	17.519027	-0.043552	2.860828
221.737186	2667.788234	17.524032	-0.043526	2.856891
221.698538	2659.802978	17.529037	-0.043514	2.852946
221.627863	2651.828623	17.534042	-0.043496	2.848998
221.437030	2643.850616	17.539047	-0.043455	2.845037
221.349528	2635.923689	17.544051	-0.043434	2.841101
221.266603	2627.938796	17.549056	-0.043413	2.837131
221.261755	2619.929888	17.554061	-0.043407	2.833148
221.154210	2611.950845	17.559066	-0.043382	2.829168
221.048504	2603.947844	17.564071	-0.043358	2.825171
221.140456	2595.984839	17.569075	-0.043370	2.821200
221.026004	2588.017971	17.574080	-0.043344	2.817209
220.930474	2580.019169	17.579085	-0.043321	2.813197
221.241073	2571.990110	17.584090	-0.043374	2.809188
221.004145	2564.037881	17.589095	-0.043325	2.805181
220.970517	2556.122693	17.594099	-0.043313	2.801198
221.074590	2548.124828	17.599104	-0.043328	2.797175
220.950837	2540.150553	17.604109	-0.043300	2.793146
220.830590	2532.155331	17.609114	-0.043272	2.789100
220.661637	2524.176199	17.614119	-0.043236	2.785053
220.817101	2516.218433	17.619123	-0.043260	2.781031
220.497328	2508.267820	17.624128	-0.043195	2.776978
220.295784	2500.303525	17.629133	-0.043153	2.772920
220.415695	2492.279091	17.634138	-0.043170	2.768844
220.519398	2484.274424	17.639143	-0.043184	2.764771
220.441032	2476.349304	17.644147	-0.043165	2.760721
220.291410	2468.393562	17.649152	-0.043132	2.756646
220.417006	2460.331345	17.654157	-0.043150	2.752527
220.406047	2452.324605	17.659162	-0.043143	2.748422
220.304499	2444.345994	17.664167	-0.043119	2.744320
220.246647	2436.420921	17.669171	-0.043104	2.740241
220.167335	2428.459327	17.674176	-0.043084	2.736137
220.077336	2420.474695	17.679181	-0.043062	2.732014
220.161382	2412.494772	17.684186	-0.043073	2.727897
220.002521	2404.521379	17.689191	-0.043038	2.723763
219.972107	2396.571362	17.694195	-0.043028	2.719643
219.950839	2388.613075	17.699200	-0.043019	2.715512
219.901312	2380.607251	17.704205	-0.043004	2.711349
219.664503	2372.651168	17.709210	-0.042955	2.707194
219.541640	2364.669821	17.714215	-0.042928	2.703026
219.763571	2356.696465	17.719219	-0.042964	2.698877
219.567300	2348.730090	17.724224	-0.042922	2.694700
219.452177	2340.730652	17.729229	-0.042896	2.690503
219.487104	2332.779762	17.734234	-0.042897	2.686336
219.582918	2324.776221	17.739239	-0.042910	2.682137
219.438003	2316.867677	17.744243	-0.042878	2.677967
219.286184	2308.880609	17.749248	-0.042845	2.673749
219.414886	2300.844361	17.754253	-0.042864	2.669516
219.339315	2292.899346	17.759258	-0.042845	2.665311
219.277738	2284.915711	17.764263	-0.042829	2.661080
219.228842	2276.976787	17.769267	-0.042814	2.656867
219.221537	2268.996060	17.774272	-0.042808	2.652628
219.032228	2261.024291	17.779277	-0.042768	2.648374
218.799145	2253.081342	17.784282	-0.042719	2.644127
218.793209	2245.098830	17.789287	-0.042713	2.639866
218.894260	2237.148426	17.794291	-0.042727	2.635623
218.842344	2229.136402	17.799296	-0.042713	2.631329
218.889852	2221.131604	17.804301	-0.042716	2.627039
218.739010	2213.202410	17.809306	-0.042683	2.622770
218.700436	2205.233466	17.814311	-0.042671	2.618479
218.792400	2197.259385	17.819315	-0.042683	2.614188
218.599405	2189.277688	17.824320	-0.042642	2.609866
218.562985	2181.314646	17.829325	-0.042631	2.605558
218.706505	2173.341219	17.834330	-0.042652	2.601249
218.711172	2165.383294	17.839335	-0.042648	2.596932
218.782350	2157.314907	17.844339	-0.042656	2.592552
218.504046	2149.268043	17.849344	-0.042600	2.588152
218.611995	2141.300433	17.854349	-0.042615	2.583815
218.520035	2133.404358	17.859354	-0.042593	2.579496
218.126811	2125.503857	17.864359	-0.042515	2.575146
218.260841	2117.502144	17.869363	-0.042534	2.570770
218.327875	2109.532366	17.874368	-0.042542	2.566400
218.273307	2101.589780	17.879373	-0.042527	2.562028
218.169303	2093.661937	17.884378	-0.042503	2.557654
218.014675	2085.699014	17.889383	-0.042469	2.553249
218.087670	2077.695355	17.894387	-0.042477	2.548830
218.073250	2069.719173	17.899392	-0.042470	2.544412
218.056315	2061.772911	17.904397	-0.042462	2.540003
217.862685	2053.837998	17.909402	-0.042421	2.535580
217.814589	2045.849985	17.914407	-0.042407	2.531131
217.864501	2037.876935	17.919411	-0.042411	2.526688
217.781227	2029.924597	17.924416	-0.042390	2.522240
217.655602	2021.983960	17.929421	-0.042362	2.517788
217.822123	2013.973172	17.934426	-0.042388	2.513309
217.586325	2005.990265	17.939431	-0.042339	2.508809
217.459763	1998.040180	17.944435	-0.042311	2.504327
217.361955	1990.100963	17.949440	-0.042287	2.499846
217.367302	1982.135914	17.954445	-0.042283	2.495349
217.463756	1974.144195	17.959450	-0.042296	2.490836
217.394084	1966.175214	17.964455	-0.042278	2.486315
217.201053	1958.248864	17.969459	-0.042238	2.481801
217.233606	1950.295383	17.974464	-0.042239	2.477280
217.256693	1942.291659	17.979469	-0.042238	2.472721
217.145744	1934.342006	17.984474	-0.042212	2.468175
216.929018	1926.381604	17.989479	-0.042167	2.463607
216.879105	1918.448578	17.994483	-0.042153	2.459058
216.844931	1910.480105	17.999488	-0.042141	2.454481
216.826346	1902.488667	18.004493	-0.042133	2.449884
216.819005	1894.540800	18.009498	-0.042127	2.445304
216.528596	1886.613984	18.014503	-0.042068	2.440706
216.548765	1878.665682	18.019507	-0.042066	2.436111
216.693931	1870.596369	18.024512	-0.042088	2.431447
216.565981	1862.631172	18.029517	-0.042059	2.426813
216.226709	1854.727719	18.034522	-0.041991	2.422189
216.259648	1846.753853	18.039527	-0.041993	2.417545
216.344908	1838.786468	18.044531	-0.042003	2.412899
216.243975	1830.819387	18.049536	-0.041980	2.408231
216.063353	1822.887994	18.054541	-0.041941	2.403567
216.263431	1814.915789	18.059546	-0.041973	2.398901
216.154293	1806.957824	18.064551	-0.041948	2.394209
216.343213	1798.969862	18.069555	-0.041978	2.389515
216.368612	1791.009324	18.074560	-0.041978	2.384814
216.318176	1783.076200	18.079565	-0.041964	2.380114
216.243708	1775.152792	18.084570	-0.041945	2.375409
215.968558	1767.192589	18.089575	-0.041889	2.370656
215.946340	1759.228874	18.094579	-0.041879	2.365912
215.813782	1751.285295	18.099584	-0.041850	2.361162
215.798294	1743.344843	18.104589	-0.041842	2.356413
215.951342	1735.343733	18.109594	-0.041865	2.351632
215.794762	1727.362255	18.114599	-0.041831	2.346828
215.695529	1719.433507	18.119603	-0.041808	2.342050
215.594123	1711.496969	18.124608	-0.041784	2.337258
215.581018	1703.526809	18.129613	-0.041777	2.332443
215.516107	1695.567535	18.134618	-0.041760	2.327620
215.562401	1687.602684	18.139623	-0.041763	2.322793
215.515466	1679.679648	18.144627	-0.041749	2.317973
215.470974	1671.717474	18.149632	-0.041736	2.313120
215.284635	1663.757726	18.154637	-0.041697	2.308246
215.396675	1655.789032	18.159642	-0.041712	2.303382
215.426472	1647.836928	18.164647	-0.041713	2.298510
215.505456	1639.903519	18.169651	-0.041723	2.293644
215.242307	1631.950391	18.174656	-0.041669	2.288726
215.200922	1624.006189	18.179661	-0.041656	2.283822
215.165974	1616.078934	18.184666	-0.041645	2.278918
214.807967	1608.138920	18.189671	-0.041573	2.273969
214.790123	1600.115585	18.194675	-0.041565	2.268985
214.673895	1592.162355	18.199680	-0.041538	2.264026
214.609260	1584.228953	18.204685	-0.041521	2.259073
214.669223	1576.288423	18.209690	-0.041527	2.254116
214.636971	1568.302221	18.214695	-0.041516	2.249111
214.492866	1560.379203	18.219699	-0.041484	2.244124
214.393754	1552.453473	18.224704	-0.041461	2.239129
214.484608	1544.497167	18.229709	-0.041473	2.234120
214.428145	1536.549397	18.234714	-0.041458	2.229092
214.452066	1528.576808	18.239719	-0.041457	2.224044
214.532394	1520.648751	18.244723	-0.041467	2.219018
214.606498	1512.695108	18.249728	-0.041476	2.213963
214.326903	1504.769987	18.254733	-0.041419	2.208884
214.228701	1496.838684	18.259738	-0.041396	2.203805
214.394686	1488.884049	18.264743	-0.041421	2.198723
214.303758	1480.962859	18.269747	-0.041400	2.193628
214.169342	1472.981258	18.274752	-0.041370	2.188478
213.909727	1465.051492	18.279757	-0.041316	2.183338
213.929987	1457.129538	18.284762	-0.041315	2.178216
213.592086	1449.201081	18.289767	-0.041247	2.173045
213.819673	1441.213655	18.294771	-0.041285	2.167876
213.720582	1433.274412	18.299776	-0.041261	2.162695
213.669476	1425.345489	18.304781	-0.041247	2.157513
213.682581	1417.416694	18.309786	-0.041244	2.152325
213.832002	1409.426654	18.314791	-0.041267	2.147097
213.693871	1401.525823	18.319795	-0.041236	2.141887
213.598040	1393.598264	18.324800	-0.041214	2.136651
213.524535	1385.661741	18.329805	-0.041195	2.131399
213.586439	1377.705574	18.334810	-0.041201	2.126133
213.504400	1369.774525	18.339815	-0.041181	2.120858
213.501105	1361.853534	18.344819	-0.041176	2.115583
213.532065	1353.845973	18.349824	-0.041176	2.110241
213.233471	1345.930060	18.354829	-0.041116	2.104914
213.287130	1338.009175	18.359834	-0.041121	2.099605
213.155127	1330.079323	18.364839	-0.041091	2.094258
213.131295	1322.134909	18.369843	-0.041082	2.088899
213.156692	1314.197498	18.374848	-0.041082	2.083535
213.080851	1306.292002	18.379853	-0.041063	2.078169
213.162778	1298.356208	18.384858	-0.041073	2.072784
212.866143	1290.434424	18.389863	-0.041013	2.067357
212.757378	1282.523078	18.394867	-0.040988	2.061941
212.800060	1274.583561	18.399872	-0.040991	2.056507
212.761239	1266.632651	18.404877	-0.040978	2.051043
212.750647	1258.711925	18.409882	-0.040971	2.045587
212.497023	1250.810534	18.414887	-0.040919	2.040106
212.469176	1242.905447	18.419891	-0.040909	2.034630
212.263145	1234.958282	18.424896	-0.040866	2.029092
212.303315	1227.002912	18.429901	-0.040868	2.023559
212.398538	1219.074515	18.434906	-0.040881	2.018034
211.888387	1211.189753	18.439911	-0.040781	2.012463
211.996204	1203.237269	18.444915	-0.040796	2.006892
212.073493	1195.294224	18.449920	-0.040806	2.001310
211.860085	1187.403812	18.454925	-0.040761	1.995719
211.838120	1179.480115	18.459930	-0.040752	1.990108
211.955017	1171.511968	18.464935	-0.040769	1.984465
211.928782	1163.617912	18.469939	-0.040759	1.978843
211.778656	1155.704935	18.474944	-0.040726	1.973178
211.639744	1147.772817	18.479949	-0.040695	1.967485
211.719120	1139.862354	18.484954	-0.040705	1.961814
211.595169	1131.959879	18.489959	-0.040677	1.956110
211.498569	1124.012319	18.494963	-0.040654	1.950360
211.729871	1116.037718	18.499968	-0.040692	1.944610
211.551983	1108.155942	18.504973	-0.040654	1.938864
211.434850	1100.266678	18.509978	-0.040627	1.933103
211.256715	1092.331918	18.514983	-0.040589	1.927285
211.252370	1084.437534	18.519987	-0.040584	1.921498
211.265466	1076.526533	18.524992	-0.040581	1.915683
211.212500	1068.593919	18.529997	-0.040566	1.909827
211.385201	1060.666629	18.535002	-0.040593	1.903982
210.938389	1052.817979	18.540007	-0.040505	1.898108
210.760396	1044.925295	18.545011	-0.040467	1.892214
211.042967	1036.947210	18.550016	-0.040515	1.886289
210.935311	1029.059569	18.555021	-0.040490	1.880369
210.887935	1021.176640	18.560026	-0.040476	1.874440
210.903688	1013.221144	18.565031	-0.040474	1.868446
210.709878	1005.334078	18.570035	-0.040433	1.862459
210.577507	997.453239	18.575040	-0.040403	1.856465
210.427180	989.545188	18.580045	-0.040371	1.850429
210.732992	981.592449	18.585050	-0.040422	1.844392
210.509461	973.734738	18.590055	-0.040376	1.838346
210.436665	965.850048	18.595059	-0.040357	1.832278
210.520847	957.917421	18.600064	-0.040368	1.826170
210.469648	950.026445	18.605069	-0.040354	1.820058
210.401701	942.156133	18.610074	-0.040336	1.813940
210.325077	934.234917	18.615079	-0.040317	1.807760
210.127215	926.382698	18.620083	-0.040275	1.801598
209.974986	918.512860	18.625088	-0.040242	1.795407
209.904196	910.552898	18.630093	-0.040224	1.789133
210.156342	902.622210	18.635098	-0.040266	1.782900
209.912023	894.764329	18.640103	-0.040215	1.776642
209.862592	886.869691	18.645107	-0.040201	1.770356
209.893145	878.970906	18.650112	-0.040202	1.764055
209.802091	871.108160	18.655117	-0.040180	1.757744
209.691636	863.242027	18.660122	-0.040155	1.751406
209.493611	855.361354	18.665127	-0.040113	1.745022
209.631073	847.475768	18.670131	-0.040133	1.738653
209.366752	839.621721	18.675136	-0.040079	1.732235
209.164473	831.736445	18.680141	-0.040037	1.725775
209.420856	823.833837	18.685146	-0.040080	1.719336
209.147193	815.987862	18.690151	-0.040024	1.712851
209.104796	808.093262	18.695155	-0.040011	1.706331
208.998745	800.222690	18.700160	-0.039986	1.699798
209.029622	792.332504	18.705165	-0.039987	1.693241
208.960085	784.459746	18.710170	-0.039969	1.686659
208.780734	776.606858	18.715175	-0.039931	1.680055
208.790986	768.748801	18.720179	-0.039928	1.673445
208.841709	760.847057	18.725184	-0.039932	1.666777
208.601530	753.011662	18.730189	-0.039883	1.660099
208.743051	745.130408	18.735194	-0.039904	1.653407
208.622754	737.257880	18.740199	-0.039877	1.646660
208.529009	729.430317	18.745203	-0.039854	1.639927
208.476233	721.559540	18.750208	-0.039840	1.633135
208.387557	713.649677	18.755213	-0.039818	1.626276
208.307886	705.820506	18.760218	-0.039799	1.619459
207.946805	698.006785	18.765223	-0.039726	1.612587
208.054023	690.124363	18.770227	-0.039741	1.605691
208.076162	682.275661	18.775232	-0.039741	1.598783
207.850607	674.446194	18.780237	-0.039694	1.591827
207.849371	666.591677	18.785242	-0.039689	1.584851
207.841985	658.742634	18.790247	-0.039682	1.577847
207.736542	650.907873	18.795251	-0.039658	1.570811
207.738477	643.060451	18.800256	-0.039653	1.563747
207.538126	635.256843	18.805261	-0.039611	1.556661
207.688095	627.375763	18.810266	-0.039634	1.549524
207.511980	619.552898	18.815271	-0.039596	1.542359
207.462623	611.730634	18.820275	-0.039582	1.535180
207.288367	603.915187	18.825280	-0.039545	1.527955
207.316890	596.068996	18.830285	-0.039545	1.520697
207.394959	588.254914	18.835290	-0.039555	1.513442
207.084309	580.452365	18.840295	-0.039492	1.506103
206.944004	572.660134	18.845299	-0.039461	1.498764
206.859749	564.834603	18.850304	-0.039441	1.491367
206.865492	557.007068	18.855309	-0.039437	1.483944
206.802661	549.213326	18.860314	-0.039420	1.476506
206.401276	541.398648	18.865319	-0.039341	1.468956
206.655362	533.535152	18.870323	-0.039383	1.461424
206.683397	525.734627	18.875328	-0.039384	1.453879
206.549249	517.931066	18.880333	-0.039354	1.446265
206.419059	510.171665	18.885338	-0.039325	1.438654
206.254300	502.382607	18.890343	-0.039289	1.430968
206.203587	494.592245	18.895347	-0.039275	1.423258
206.101300	486.817491	18.900352	-0.039251	1.415513
206.028046	479.022558	18.905357	-0.039232	1.407710
206.054318	471.242860	18.910362	-0.039232	1.399895
206.108370	463.441926	18.915367	-0.039238	1.392020
206.099705	455.655236	18.920371	-0.039231	1.384104
205.848400	447.918612	18.925376	-0.039179	1.376152
205.766616	440.142831	18.930381	-0.039159	1.368142
205.787087	432.381670	18.935386	-0.039158	1.360118
205.631353	424.637504	18.940391	-0.039125	1.352034
205.433906	416.906105	18.945395	-0.039083	1.343907
205.281930	409.166042	18.950400	-0.039050	1.335729
205.233396	401.400755	18.955405	-0.039036	1.327493
205.222785	393.664740	18.960410	-0.039029	1.319243
205.016110	385.871590	18.965415	-0.038986	1.310844
205.293448	378.041160	18.970419	-0.039032	1.302439
205.052664	370.352493	18.975424	-0.038983	1.294038
204.892917	362.635863	18.980429	-0.038948	1.285568
204.748624	354.957522	18.985434	-0.038917	1.277085
204.936655	347.197532	18.990439	-0.038947	1.268518
204.665000	339.533695	18.995443	-0.038891	1.259914
204.375417	331.872388	19.000448	-0.038833	1.251249
204.291653	324.176156	19.005453	-0.038812	1.242524
204.300043	316.479469	19.010458	-0.038809	1.233754
204.008398	308.800926	19.015463	-0.038750	1.224884
203.922730	301.128345	19.020467	-0.038729	1.215996
204.188382	293.392223	19.025472	-0.038774	1.207039
203.850539	285.776435	19.030477	-0.038706	1.198036
203.860982	278.103177	19.035482	-0.038703	1.188966
203.647739	270.468687	19.040487	-0.038659	1.179827
203.551740	262.832201	19.045491	-0.038636	1.170639
203.470083	255.189027	19.050496	-0.038616	1.161373
203.473164	247.534571	19.055501	-0.038612	1.152036
203.599048	239.857913	19.060506	-0.038631	1.142621
203.137239	232.297193	19.065511	-0.038540	1.133147
202.967232	224.701370	19.070515	-0.038504	1.123612
202.969538	217.096191	19.075520	-0.038499	1.114021
202.805854	209.505302	19.080525	-0.038464	1.104328
202.573796	201.958086	19.085530	-0.038416	1.094590
202.351143	194.388578	19.090535	-0.038370	1.084738
202.721606	186.755601	19.095539	-0.038434	1.074847
202.303283	179.244492	19.100544	-0.038352	1.064845
202.083720	171.720353	19.105549	-0.038306	1.054776
202.161369	164.157109	19.110554	-0.038316	1.044627
201.953129	156.657694	19.115559	-0.038272	1.034398
201.874079	149.137763	19.120563	-0.038253	1.024069
201.724353	141.653101	19.125568	-0.038220	1.013666
201.592029	134.166749	19.130573	-0.038191	1.003158
201.449143	126.696474	19.135578	-0.038160	0.992559
201.297399	119.212216	19.140583	-0.038127	0.981823
201.204411	111.767174	19.145587	-0.038105	0.971040
201.012790	104.347283	19.150592	-0.038065	0.960147
200.807091	96.941507	19.155597	-0.038022	0.949147
200.821296	89.521863	19.160602	-0.038020	0.938054
200.378431	82.185085	19.165607	-0.037933	0.926833
200.175267	74.840778	19.170611	-0.037890	0.915528
200.119651	67.459269	19.175616	-0.037875	0.904063
199.637855	60.410799	19.180621	-0.037781	0.892859