Thu Mar 11 19:16:06 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.325998	0.029243	0.000000	0.000039	0.724882

0.264528	0.044975	0.005005	0.000050	0.724892
0.507997	-0.003075	0.010010	0.000004	0.724883
0.473660	0.005513	0.015014	0.000010	0.724888
0.382348	-0.001647	0.020019	0.000027	0.724843
0.506159	-0.155351	0.025024	0.000004	0.724586
0.555709	-0.158907	0.030029	-0.000005	0.724597
0.330292	-0.123281	0.035034	0.000036	0.724588
0.408409	-0.134635	0.040038	0.000021	0.724594
0.658423	-0.180220	0.045043	-0.000025	0.724592
0.540074	-0.163216	0.050048	-0.000004	0.724585
0.426906	-0.136487	0.055053	0.000017	0.724598
0.356470	-0.129450	0.060058	0.000030	0.724588
0.523573	-0.156685	0.065062	-0.000001	0.724593
0.347216	-0.124928	0.070067	0.000031	0.724594
0.498820	-0.155187	0.075072	0.000003	0.724588
0.497381	-0.176104	0.080077	0.000003	0.724547
0.396437	-0.307600	0.085082	0.000022	0.724255
0.337312	-0.293046	0.090086	0.000032	0.724264
0.412752	-0.306635	0.095091	0.000018	0.724264
0.485920	-0.323128	0.100096	0.000004	0.724257
0.238482	-0.274211	0.105101	0.000050	0.724267
0.263297	-0.283172	0.110106	0.000045	0.724259
0.355397	-0.385856	0.115110	0.000028	0.724091
0.462937	-0.474496	0.120115	0.000008	0.723955
0.274974	-0.443700	0.125120	0.000042	0.723950
0.379108	-0.458174	0.130125	0.000023	0.723959
0.341603	-0.455759	0.135130	0.000029	0.723951
0.269151	-0.532257	0.140134	0.000043	0.723776
0.364190	-0.620513	0.145139	0.000025	0.723637
0.427369	-0.634270	0.150144	0.000013	0.723632
0.507281	-0.644713	0.155149	-0.000002	0.723640
0.431813	-0.694196	0.160154	0.000011	0.723517
0.543788	-0.802482	0.165158	-0.000010	0.723345
0.415287	-0.777771	0.170163	0.000014	0.723349
0.198954	-0.743990	0.175168	0.000054	0.723340
0.243148	-0.866732	0.180173	0.000046	0.723115
0.252048	-0.926336	0.185178	0.000044	0.723002
0.201939	-0.917414	0.190182	0.000053	0.723002
0.359316	-0.983075	0.195187	0.000023	0.722929
0.374209	-1.108132	0.200192	0.000020	0.722689
0.398974	-1.108444	0.205197	0.000016	0.722698
0.443322	-1.151698	0.210202	0.000007	0.722629
0.410247	-1.277983	0.215206	0.000013	0.722370
0.431048	-1.280693	0.220211	0.000009	0.722372
0.312514	-1.316434	0.225216	0.000031	0.722261
0.606994	-1.459887	0.230221	-0.000024	0.722083
0.531415	-1.452350	0.235226	-0.000010	0.722072
0.400566	-1.548253	0.240230	0.000014	0.721838
0.339033	-1.583694	0.245235	0.000025	0.721747
0.307444	-1.611633	0.250240	0.000031	0.721682
0.106922	-1.697803	0.255245	0.000068	0.721443
0.138672	-1.708261	0.260250	0.000062	0.721434
0.198516	-1.823446	0.265254	0.000050	0.721229
0.281866	-1.892824	0.270259	0.000035	0.721122
0.210348	-1.922711	0.275264	0.000048	0.721038
0.518063	-2.056270	0.280269	-0.000010	0.720884
0.464788	-2.072730	0.285274	0.000000	0.720833
0.131273	-2.161603	0.290278	0.000062	0.720542
0.310183	-2.192829	0.295283	0.000028	0.720544
0.427814	-2.372606	0.300288	0.000006	0.720232
0.130774	-2.323117	0.305293	0.000061	0.720225
0.116220	-2.469615	0.310298	0.000064	0.719932
0.319292	-2.521787	0.315302	0.000026	0.719901
0.070110	-2.607027	0.320307	0.000072	0.719646
-2.751764	-2.130022	0.325312	0.000597	0.719596
-2.553316	-2.206270	0.330317	0.000560	0.719516
-4.333597	-2.017442	0.335322	0.000891	0.719264
-3.763574	-2.117338	0.340326	0.000785	0.719268
-3.981842	-2.076329	0.345331	0.000825	0.719272
-4.681552	-2.049665	0.350336	0.000955	0.719080
-4.989453	-2.053785	0.355341	0.001012	0.718964
-5.028730	-2.050984	0.360346	0.001019	0.718956
-5.449402	-1.975707	0.365350	0.001097	0.718957
-5.014596	-2.074352	0.370355	0.001016	0.718916
-5.943149	-2.051328	0.375360	0.001189	0.718635
-6.148969	-2.008305	0.380365	0.001227	0.718648
-6.429766	-1.962684	0.385370	0.001279	0.718640
-6.154989	-2.010793	0.390374	0.001227	0.718642
-5.820681	-2.097265	0.395379	0.001165	0.718590
-7.166409	-1.980697	0.400384	0.001415	0.718347
-6.818330	-2.036290	0.405389	0.001350	0.718360
-7.016629	-2.005321	0.410394	0.001387	0.718352
-7.083563	-1.992886	0.415398	0.001399	0.718353
-7.019490	-2.004615	0.420403	0.001387	0.718353
-7.557583	-2.039434	0.425408	0.001487	0.718096
-8.049160	-1.988468	0.430413	0.001578	0.718024
-8.070737	-1.988695	0.435418	0.001582	0.718016
-8.062058	-1.989966	0.440422	0.001580	0.718017
-8.045561	-1.992352	0.445427	0.001577	0.718019
-8.078377	-1.989550	0.450432	0.001582	0.718013
-7.986705	-2.105823	0.455437	0.001565	0.717816
-9.233905	-1.943316	0.460442	0.001797	0.717699
-9.220953	-1.943294	0.465446	0.001794	0.717704
-8.957471	-1.990660	0.470451	0.001745	0.717704
-8.922625	-1.999750	0.475456	0.001738	0.717698
-8.951273	-1.991094	0.480461	0.001744	0.717706
-9.284228	-1.947192	0.485466	0.001805	0.717676
-9.646741	-2.032059	0.490470	0.001873	0.717381
-9.571732	-2.044355	0.495475	0.001858	0.717384
-10.467806	-1.889287	0.500480	0.002025	0.717375
-9.922246	-1.982555	0.505485	0.001923	0.717383
-9.880957	-1.992950	0.510490	0.001915	0.717378
-10.257571	-1.925474	0.515494	0.001985	0.717379
-10.106956	-1.968684	0.520499	0.001957	0.717347
-10.788437	-1.985654	0.525504	0.002083	0.717074
-10.387208	-2.050456	0.530509	0.002008	0.717088
-10.955595	-1.954777	0.535514	0.002114	0.717077
-10.952259	-1.954347	0.540518	0.002113	0.717080
-10.731190	-1.992069	0.545523	0.002072	0.717083
-10.903901	-1.965370	0.550528	0.002104	0.717076
-10.846027	-2.023772	0.555533	0.002093	0.716981
-11.725782	-1.983147	0.560538	0.002256	0.716752
-11.804608	-1.969344	0.565542	0.002271	0.716752
-11.920031	-1.946932	0.570547	0.002292	0.716756
-11.833816	-1.967496	0.575552	0.002276	0.716746
-11.749318	-1.978171	0.580557	0.002260	0.716755
-12.279881	-1.887135	0.585562	0.002358	0.716749
-11.955277	-1.943380	0.590566	0.002297	0.716752
-11.810087	-2.103893	0.595571	0.002270	0.716486
-12.992842	-1.916388	0.600576	0.002490	0.716441
-13.167808	-1.880532	0.605581	0.002522	0.716451
-12.513238	-2.001626	0.610586	0.002400	0.716442
-12.668848	-1.973081	0.615590	0.002429	0.716444
-12.903168	-1.929293	0.620595	0.002472	0.716449
-12.842159	-1.946114	0.625600	0.002461	0.716438
-12.595685	-2.093991	0.630605	0.002415	0.716232
-13.636791	-1.963700	0.635610	0.002608	0.716123
-13.892125	-1.917193	0.640614	0.002656	0.716126
-13.379634	-2.005966	0.645619	0.002560	0.716131
-13.730384	-1.946757	0.650624	0.002625	0.716125
-13.628389	-1.961302	0.655629	0.002606	0.716133
-13.678535	-1.956981	0.660634	0.002615	0.716124
-13.788431	-2.012061	0.665638	0.002635	0.715977
-14.523648	-1.928674	0.670643	0.002772	0.715883
-14.319583	-1.968770	0.675648	0.002733	0.715876
-14.292173	-1.970464	0.680653	0.002728	0.715883
-14.640496	-1.911685	0.685658	0.002793	0.715877
-14.457637	-1.942685	0.690662	0.002758	0.715880
-14.112875	-2.004023	0.695667	0.002694	0.715881
-14.722493	-2.040693	0.700672	0.002807	0.715594
-15.670061	-1.896418	0.705677	0.002983	0.715545
-15.253139	-1.974707	0.710682	0.002905	0.715538
-15.065320	-2.005491	0.715686	0.002870	0.715544
-15.391157	-1.946030	0.720691	0.002931	0.715547
-15.449449	-1.941080	0.725696	0.002941	0.715537
-14.978729	-2.019977	0.730701	0.002853	0.715547
-15.639151	-2.048782	0.735706	0.002976	0.715257
-16.537345	-1.904395	0.740710	0.003143	0.715227
-16.020128	-1.994059	0.745715	0.003047	0.715232
-15.999318	-2.001073	0.750720	0.003042	0.715226
-16.249569	-1.953936	0.755725	0.003089	0.715231
-16.439863	-1.923343	0.760730	0.003124	0.715225
-16.503506	-1.911889	0.765734	0.003136	0.715226
-16.522238	-2.015643	0.770739	0.003139	0.715014
-17.471457	-1.905068	0.775744	0.003315	0.714898
-16.799523	-2.019899	0.780749	0.003190	0.714908
-17.022010	-1.982192	0.785754	0.003231	0.714905
-17.682568	-1.865065	0.790758	0.003354	0.714904
-16.966411	-1.992297	0.795763	0.003220	0.714906
-17.140565	-1.964066	0.800768	0.003252	0.714901
-17.507173	-1.968244	0.805773	0.003320	0.714763
-18.186983	-1.928993	0.810778	0.003447	0.714601
-17.707935	-2.012728	0.815782	0.003357	0.714605
-18.083898	-1.944257	0.820787	0.003427	0.714608
-18.573537	-1.862334	0.825792	0.003518	0.714598
-17.898709	-1.976663	0.830797	0.003392	0.714610
-18.001296	-1.963421	0.835802	0.003411	0.714601
-18.559022	-1.861507	0.840806	0.003514	0.714606
-18.581604	-2.019060	0.845811	0.003519	0.714286
-18.885105	-1.973125	0.850816	0.003575	0.714270
-19.017031	-1.945773	0.855821	0.003599	0.714278
-18.802496	-1.986786	0.860826	0.003559	0.714273
-19.228788	-1.911155	0.865830	0.003638	0.714273
-19.048779	-1.941341	0.870835	0.003604	0.714277
-19.001556	-1.952665	0.875840	0.003595	0.714272
-19.216962	-2.039691	0.880845	0.003635	0.714023
-20.220504	-1.891340	0.885850	0.003822	0.713963
-20.303018	-1.875502	0.890854	0.003837	0.713966
-19.586166	-2.001728	0.895859	0.003703	0.713970
-20.100239	-1.915955	0.900864	0.003799	0.713958
-20.146571	-1.899769	0.905869	0.003807	0.713975
-19.986415	-1.932429	0.910874	0.003777	0.713967
-19.906285	-1.995563	0.915878	0.003762	0.713870
-20.740249	-1.956528	0.920883	0.003917	0.713653
-21.169710	-1.884097	0.925888	0.003996	0.713645
-21.177788	-1.878735	0.930893	0.003998	0.713654
-20.794220	-1.950139	0.935898	0.003926	0.713648
-20.791552	-1.950852	0.940902	0.003925	0.713648
-20.878393	-1.933145	0.945907	0.003941	0.713653
-20.932801	-1.929224	0.950912	0.003951	0.713642
-21.193466	-2.007324	0.955917	0.003999	0.713395
-21.982640	-1.886967	0.960922	0.004146	0.713355
-21.861878	-1.908604	0.965926	0.004123	0.713355
-21.545594	-1.962448	0.970931	0.004064	0.713361
-21.836967	-1.915127	0.975936	0.004118	0.713352
-21.605004	-1.953359	0.980941	0.004075	0.713359
-21.716102	-1.936235	0.985946	0.004095	0.713354
-22.617734	-1.909100	0.990950	0.004263	0.713089
-22.838862	-1.904062	0.995955	0.004304	0.713021
-22.773786	-1.918837	1.000960	0.004291	0.713015
-22.673543	-1.933327	1.005965	0.004272	0.713022
-23.310048	-1.824706	1.010970	0.004391	0.713013
-22.822774	-1.911371	1.015974	0.004300	0.713014
-22.373913	-1.989310	1.020979	0.004216	0.713018
-23.210447	-1.844813	1.025984	0.004371	0.713010
-23.667806	-1.892844	1.030989	0.004456	0.712752
-23.685031	-1.915378	1.035994	0.004459	0.712702
-23.898489	-1.878013	1.040998	0.004499	0.712701
-23.883871	-1.877798	1.046003	0.004496	0.712707
-23.919471	-1.876711	1.051008	0.004502	0.712697
-23.702540	-1.912975	1.056013	0.004462	0.712702
-23.694521	-1.915426	1.061018	0.004460	0.712701
-23.752838	-1.922992	1.066022	0.004470	0.712666
-24.200076	-1.986671	1.071027	0.004553	0.712381
-24.504725	-1.936661	1.076032	0.004610	0.712372
-24.964978	-1.848543	1.081037	0.004695	0.712385
-24.586509	-1.919979	1.086042	0.004625	0.712378
-24.881741	-1.867533	1.091046	0.004679	0.712378
-24.769043	-1.884091	1.096051	0.004658	0.712385
-24.453442	-1.944991	1.101056	0.004599	0.712376
-24.904135	-1.987820	1.106061	0.004683	0.712132
-25.980150	-1.822100	1.111066	0.004883	0.712080
-25.969192	-1.825074	1.116070	0.004881	0.712079
-25.082387	-1.979803	1.121075	0.004715	0.712086
-25.861638	-1.845537	1.126080	0.004860	0.712077
-25.590107	-1.889106	1.131085	0.004809	0.712087
-25.345476	-1.935088	1.136090	0.004764	0.712083
-25.392045	-2.012362	1.141094	0.004772	0.711913
-26.627899	-1.869201	1.146099	0.005002	0.711760
-26.455780	-1.905355	1.151104	0.004969	0.711749
-26.253851	-1.937973	1.156109	0.004932	0.711756
-26.524345	-1.892008	1.161114	0.004982	0.711752
-26.470829	-1.901391	1.166118	0.004972	0.711753
-26.204659	-1.945613	1.171123	0.004922	0.711760
-26.837569	-1.900321	1.176128	0.005039	0.711626
-27.666676	-1.840050	1.181133	0.005193	0.711452
-27.181547	-1.927401	1.186138	0.005103	0.711451
-27.563865	-1.862173	1.191142	0.005174	0.711445
-27.414507	-1.884878	1.196147	0.005146	0.711454
-27.270726	-1.916254	1.201152	0.005119	0.711443
-27.171468	-1.929875	1.206157	0.005100	0.711451
-27.551141	-1.864414	1.211162	0.005170	0.711447
-28.150726	-1.915699	1.216166	0.005282	0.711132
-27.885421	-1.960711	1.221171	0.005232	0.711137
-28.439851	-1.866962	1.226176	0.005335	0.711128
-28.514114	-1.849742	1.231181	0.005349	0.711136
-28.308981	-1.888295	1.236186	0.005310	0.711133
-28.276278	-1.893265	1.241190	0.005304	0.711135
-28.180403	-1.907811	1.246195	0.005286	0.711140
-28.476155	-1.951979	1.251200	0.005341	0.710947
-29.181976	-1.864326	1.256205	0.005472	0.710872
-28.939555	-1.911439	1.261210	0.005426	0.710864
-29.352488	-1.840046	1.266214	0.005503	0.710861
-29.057675	-1.889497	1.271219	0.005448	0.710867
-29.139197	-1.878336	1.276224	0.005463	0.710861
-29.001764	-1.897943	1.281229	0.005437	0.710871
-29.099713	-2.015037	1.286234	0.005455	0.710603
-30.037360	-1.887222	1.291238	0.005629	0.710525
-30.170651	-1.859799	1.296243	0.005654	0.710533
-30.336487	-1.835407	1.301248	0.005685	0.710523
-29.893567	-1.909418	1.306253	0.005602	0.710533
-30.149047	-1.869013	1.311258	0.005649	0.710524
-30.316038	-1.838398	1.316262	0.005680	0.710526
-29.771686	-2.016015	1.321267	0.005579	0.710365
-30.808872	-1.910950	1.326272	0.005771	0.710206
-30.833827	-1.903304	1.331277	0.005776	0.710213
-30.955467	-1.883310	1.336282	0.005798	0.710210
-30.985557	-1.878068	1.341286	0.005803	0.710210
-30.868732	-1.895845	1.346291	0.005781	0.710217
-31.290171	-1.825822	1.351296	0.005860	0.710207
-30.916390	-1.977457	1.356301	0.005790	0.710038
-31.825371	-1.893050	1.361306	0.005959	0.709883
-32.029083	-1.855539	1.366310	0.005996	0.709886
-31.903348	-1.875686	1.371315	0.005973	0.709891
-31.785599	-1.900149	1.376320	0.005951	0.709885
-31.830726	-1.888909	1.381325	0.005959	0.709892
-31.784739	-1.899763	1.386330	0.005950	0.709887
-31.840034	-1.951200	1.391334	0.005960	0.709765
-32.654890	-1.892392	1.396339	0.006112	0.709592
-32.761117	-1.876586	1.401344	0.006131	0.709587
-32.494210	-1.921231	1.406349	0.006081	0.709593
-32.743836	-1.879518	1.411354	0.006127	0.709588
-32.970485	-1.839792	1.416358	0.006169	0.709587
-32.619339	-1.900737	1.421363	0.006104	0.709591
-32.501039	-1.972317	1.426368	0.006081	0.709490
-33.701989	-1.873212	1.431373	0.006305	0.709261
-33.656624	-1.884227	1.436378	0.006296	0.709255
-33.551453	-1.902350	1.441382	0.006276	0.709257
-33.386508	-1.930386	1.446387	0.006245	0.709260
-33.839203	-1.852518	1.451392	0.006329	0.709255
-33.890010	-1.838982	1.456397	0.006339	0.709265
-33.594250	-1.897938	1.461402	0.006283	0.709252
-34.424619	-1.901795	1.466406	0.006438	0.708949
-34.466689	-1.890754	1.471411	0.006445	0.708957
-34.594674	-1.873016	1.476416	0.006469	0.708947
-34.423294	-1.900251	1.481421	0.006437	0.708954
-34.758986	-1.842531	1.486426	0.006499	0.708950
-34.720634	-1.850112	1.491430	0.006491	0.708949
-34.515826	-1.884474	1.496435	0.006453	0.708954
-34.912575	-1.909269	1.501440	0.006527	0.708763
-35.351035	-1.892858	1.506445	0.006608	0.708640
-34.803837	-1.993195	1.511450	0.006506	0.708635
-35.801567	-1.817440	1.516454	0.006691	0.708631
-35.601267	-1.849442	1.521459	0.006654	0.708639
-35.039337	-1.953651	1.526464	0.006549	0.708632
-35.376749	-1.889934	1.531469	0.006612	0.708639
-35.923527	-1.898501	1.536474	0.006713	0.708427
-36.215249	-1.890177	1.541478	0.006767	0.708340
-35.763883	-1.964515	1.546483	0.006683	0.708353
-36.422957	-1.854061	1.551488	0.006805	0.708339
-36.360133	-1.860667	1.556493	0.006793	0.708349
-35.957252	-1.935516	1.561498	0.006718	0.708343
-36.337469	-1.869039	1.566502	0.006789	0.708341
-36.452084	-1.987641	1.571507	0.006810	0.708063
-37.101833	-1.902010	1.576512	0.006931	0.708003
-37.181245	-1.883812	1.581517	0.006945	0.708012
-37.021885	-1.915296	1.586522	0.006915	0.708006
-37.479491	-1.835022	1.591526	0.007000	0.708004
-37.153587	-1.889222	1.596531	0.006939	0.708012
-37.300792	-1.866649	1.601536	0.006966	0.708005
-37.360749	-1.962467	1.606541	0.006977	0.707792
-38.089444	-1.881506	1.611546	0.007113	0.707695
-38.326063	-1.840659	1.616550	0.007157	0.707692
-38.200893	-1.859588	1.621555	0.007133	0.707700
-38.338577	-1.840228	1.626560	0.007158	0.707690
-38.074167	-1.883431	1.631565	0.007109	0.707698
-38.220122	-1.859599	1.636570	0.007136	0.707694
-38.244077	-1.891366	1.641574	0.007140	0.707622
-38.582121	-1.954088	1.646579	0.007203	0.707376
-39.006925	-1.881640	1.651584	0.007282	0.707370
-39.371398	-1.813607	1.656589	0.007349	0.707377
-38.953014	-1.891181	1.661594	0.007271	0.707371
-39.136714	-1.860193	1.666598	0.007305	0.707368
-39.371718	-1.813992	1.671603	0.007348	0.707377
-39.313900	-1.829398	1.676608	0.007337	0.707368
-39.283176	-1.942328	1.681613	0.007332	0.707152
-40.061837	-1.842962	1.686618	0.007476	0.707074
-40.130443	-1.830971	1.691622	0.007489	0.707074
-39.728265	-1.898776	1.696627	0.007414	0.707082
-40.207270	-1.818647	1.701632	0.007503	0.707072
-39.974493	-1.855674	1.706637	0.007459	0.707081
-39.735340	-1.899240	1.711642	0.007414	0.707080
-40.259571	-1.905820	1.716646	0.007512	0.706880
-41.130715	-1.813227	1.721651	0.007674	0.706754
-40.882554	-1.863724	1.726656	0.007627	0.706742
-40.674063	-1.896075	1.731661	0.007588	0.706752
-41.130994	-1.817428	1.736666	0.007673	0.706747
-40.991729	-1.844200	1.741670	0.007647	0.706744
-40.401863	-1.945387	1.746675	0.007537	0.706752
-40.755043	-1.941537	1.751680	0.007602	0.706634
-42.068867	-1.804579	1.756685	0.007846	0.706439
-41.500900	-1.907537	1.761690	0.007741	0.706436
-41.639002	-1.883119	1.766694	0.007766	0.706436
-41.534865	-1.896676	1.771699	0.007746	0.706447
-41.909261	-1.835109	1.776704	0.007816	0.706437
-41.674017	-1.875261	1.781709	0.007772	0.706441
-41.434565	-1.969605	1.786714	0.007727	0.706337
-42.637019	-1.865653	1.791718	0.007951	0.706116
-42.050760	-1.964536	1.796723	0.007841	0.706128
-42.461037	-1.896801	1.801728	0.007917	0.706117
-42.756718	-1.840604	1.806733	0.007972	0.706125
-42.557349	-1.877158	1.811738	0.007935	0.706123
-42.715584	-1.850665	1.816742	0.007964	0.706120
-42.648282	-1.923303	1.821747	0.007951	0.705999
-43.500523	-1.843886	1.826752	0.008110	0.705853
-42.836515	-1.958301	1.831757	0.007986	0.705862
-43.180402	-1.898246	1.836762	0.008050	0.705860
-43.768191	-1.795216	1.841766	0.008159	0.705857
-42.854665	-1.955081	1.846771	0.007988	0.705863
-43.216159	-1.895458	1.851776	0.008055	0.705854
-43.748524	-1.957501	1.856781	0.008154	0.705539
-44.192536	-1.887585	1.861786	0.008237	0.705521
-44.273776	-1.874815	1.866790	0.008252	0.705518
-44.064365	-1.908699	1.871795	0.008212	0.705525
-44.441909	-1.846831	1.876800	0.008282	0.705515
-44.103138	-1.902225	1.881805	0.008219	0.705525
-43.986676	-1.950182	1.886810	0.008197	0.705471
-45.100823	-1.884382	1.891814	0.008404	0.705204
-44.851323	-1.925688	1.896819	0.008358	0.705211
-45.186234	-1.870951	1.901824	0.008420	0.705202
-45.106561	-1.880546	1.906829	0.008405	0.705211
-44.732209	-1.949692	1.911834	0.008335	0.705207
-45.181736	-1.871343	1.916838	0.008418	0.705204
-45.384007	-1.867505	1.921843	0.008456	0.705139
-46.066622	-1.873567	1.926848	0.008582	0.704883
-45.727614	-1.931995	1.931853	0.008519	0.704887
-45.956961	-1.891811	1.936858	0.008562	0.704886
-46.512245	-1.796117	1.941862	0.008665	0.704880
-45.589443	-1.956761	1.946867	0.008493	0.704888
-45.767609	-1.929111	1.951872	0.008526	0.704881
-46.015255	-1.917169	1.956877	0.008571	0.704816
-46.752825	-1.898806	1.961882	0.008708	0.704589
-46.656832	-1.918986	1.966886	0.008690	0.704583
-46.658515	-1.916367	1.971891	0.008690	0.704588
-47.030051	-1.852344	1.976896	0.008759	0.704584
-46.886014	-1.875278	1.981901	0.008732	0.704590
-46.639995	-1.921352	1.986906	0.008686	0.704586
-46.847234	-1.943554	1.991910	0.008725	0.704467
-47.491567	-1.932887	1.996915	0.008844	0.704258
-47.766034	-1.885694	2.001920	0.008895	0.704255

-47.555785	-1.925088	2.011917	0.008856	0.704252
-47.811712	-1.879238	2.021914	0.008903	0.704253
-47.758879	-1.887079	2.031910	0.008892	0.704258
-47.922854	-1.859057	2.041907	0.008922	0.704256
-47.650639	-1.906669	2.051904	0.008871	0.704259
-47.899621	-1.863879	2.061901	0.008917	0.704257
-47.715394	-1.897704	2.071898	0.008882	0.704256
-47.665337	-1.906949	2.081894	0.008872	0.704256
-47.926800	-1.860693	2.091891	0.008921	0.704256
-47.870230	-1.872108	2.101888	0.008910	0.704254
-47.633531	-1.914008	2.111885	0.008865	0.704256
-47.698154	-1.902420	2.121882	0.008877	0.704257
-47.706779	-1.901823	2.131878	0.008878	0.704256
-47.521443	-1.840314	2.141875	0.008843	0.704448
-46.820218	-1.896466	2.151872	0.008712	0.704587
-47.260313	-1.818947	2.161869	0.008793	0.704586
-46.966172	-1.871203	2.171866	0.008738	0.704588
-47.049162	-1.821704	2.181862	0.008753	0.704659
-46.226376	-1.855157	2.191859	0.008599	0.704888
-46.046694	-1.889800	2.201856	0.008565	0.704883
-46.301829	-1.843744	2.211853	0.008612	0.704886
-46.203771	-1.816339	2.221850	0.008593	0.704977
-45.279558	-1.867273	2.231846	0.008421	0.705207
-45.271999	-1.869174	2.241843	0.008419	0.705207
-45.094020	-1.900719	2.251840	0.008385	0.705208
-45.273811	-1.791533	2.261837	0.008418	0.705364
-44.090299	-1.925132	2.271834	0.008197	0.705521
-44.421265	-1.865480	2.281830	0.008258	0.705523
-44.383953	-1.871870	2.291827	0.008251	0.705525
-43.827579	-1.834208	2.301824	0.008147	0.705801
-43.714118	-1.826040	2.311821	0.008125	0.705859
-43.469636	-1.870253	2.321818	0.008079	0.705859
-43.387959	-1.849616	2.331814	0.008064	0.705931
-42.698137	-1.876437	2.341811	0.007935	0.706125
-42.544706	-1.904613	2.351808	0.007906	0.706124
-42.962980	-1.829439	2.361805	0.007983	0.706126
-41.945591	-1.894479	2.371802	0.007793	0.706361
-42.018788	-1.840957	2.381798	0.007806	0.706443
-41.881760	-1.866948	2.391795	0.007780	0.706441
-41.828873	-1.841419	2.401792	0.007770	0.706512
-41.064230	-1.861180	2.411789	0.007627	0.706748
-40.824447	-1.903308	2.421786	0.007582	0.706750
-41.117286	-1.850923	2.431782	0.007636	0.706751
-40.463530	-1.837212	2.441779	0.007514	0.707014
-40.303690	-1.833948	2.451776	0.007483	0.707078
-40.186167	-1.855645	2.461773	0.007461	0.707078
-39.851677	-1.846327	2.471770	0.007398	0.707217
-39.202912	-1.883199	2.481766	0.007277	0.707376
-38.902672	-1.938477	2.491763	0.007220	0.707374
-39.256298	-1.877127	2.501760	0.007286	0.707371
-38.545686	-1.879931	2.511757	0.007153	0.707621
-38.361840	-1.875188	2.521754	0.007118	0.707697
-38.289733	-1.888555	2.531750	0.007104	0.707697
-38.219147	-1.873246	2.541747	0.007091	0.707754
-37.669442	-1.844918	2.551744	0.006988	0.708008
-37.522922	-1.871704	2.561741	0.006960	0.708007
-37.578217	-1.862558	2.571738	0.006970	0.708007
-36.794486	-1.855419	2.581734	0.006823	0.708302
-36.337944	-1.914100	2.591731	0.006738	0.708349
-36.778566	-1.835652	2.601728	0.006819	0.708349
-36.530112	-1.839886	2.611725	0.006773	0.708431
-35.631919	-1.897729	2.621722	0.006605	0.708636
-35.738550	-1.878420	2.631718	0.006624	0.708638
-35.629120	-1.898165	2.641715	0.006603	0.708638
-35.313571	-1.828439	2.651712	0.006544	0.708892
-34.776700	-1.894621	2.661709	0.006444	0.708952
-34.922822	-1.870108	2.671706	0.006470	0.708950
-34.740585	-1.845910	2.681702	0.006436	0.709064
-33.785056	-1.918789	2.691699	0.006258	0.709260
-33.973574	-1.885940	2.701696	0.006292	0.709259
-34.168818	-1.852049	2.711693	0.006328	0.709258
-33.418177	-1.834157	2.721690	0.006188	0.709563
-33.252559	-1.848793	2.731686	0.006156	0.709594
-33.065334	-1.883847	2.741683	0.006121	0.709591
-33.150976	-1.787623	2.751680	0.006136	0.709754
-32.326103	-1.868579	2.761677	0.005982	0.709887
-32.641675	-1.812385	2.771674	0.006041	0.709888
-32.190004	-1.849180	2.781670	0.005956	0.709976
-31.520365	-1.848325	2.791667	0.005831	0.710217
-31.495815	-1.854975	2.801664	0.005826	0.710214
-31.578547	-1.840902	2.811661	0.005841	0.710213
-30.950012	-1.808813	2.821658	0.005723	0.710502
-30.620704	-1.852440	2.831654	0.005661	0.710533
-30.491183	-1.876193	2.841651	0.005637	0.710533
-30.488476	-1.801627	2.851648	0.005636	0.710684
-29.407732	-1.901891	2.861645	0.005434	0.710869
-29.760827	-1.838544	2.871642	0.005499	0.710871
-29.624437	-1.863873	2.881638	0.005473	0.710870
-29.322698	-1.807669	2.891635	0.005417	0.711090
-29.057181	-1.833138	2.901632	0.005367	0.711135
-28.864924	-1.867834	2.911629	0.005331	0.711135
-28.690335	-1.819796	2.921626	0.005297	0.711294
-27.850554	-1.889568	2.931622	0.005141	0.711454
-28.021290	-1.859188	2.941619	0.005172	0.711455
-28.306861	-1.793927	2.951616	0.005225	0.711484
-27.350562	-1.827918	2.961613	0.005046	0.711757
-27.324281	-1.832411	2.971610	0.005041	0.711759
-27.120042	-1.868104	2.981606	0.005002	0.711761
-26.728789	-1.810488	2.991603	0.004929	0.712016
-26.272754	-1.856302	3.001600	0.004843	0.712087
-26.200671	-1.869700	3.011597	0.004829	0.712087
-26.302842	-1.808751	3.021594	0.004848	0.712173
-25.416791	-1.860329	3.031590	0.004683	0.712386
-25.530045	-1.840075	3.041587	0.004703	0.712387
-25.515560	-1.844622	3.051584	0.004700	0.712384
-24.830767	-1.825334	3.061581	0.004572	0.712667
-24.636213	-1.839947	3.071578	0.004535	0.712707
-24.383722	-1.885332	3.081574	0.004488	0.712708
-24.659896	-1.777559	3.091571	0.004539	0.712825
-23.576017	-1.870952	3.101568	0.004336	0.713025
-23.944125	-1.807685	3.111565	0.004404	0.713021
-23.798743	-1.832376	3.121562	0.004377	0.713024
-22.904997	-1.824208	3.131558	0.004210	0.713358
-22.885656	-1.827305	3.141555	0.004206	0.713360
-22.650299	-1.869360	3.151552	0.004161	0.713361
-22.648462	-1.811301	3.161549	0.004161	0.713478
-21.724363	-1.889446	3.171546	0.003988	0.713651
-21.825536	-1.871071	3.181542	0.004006	0.713652
-22.056306	-1.829920	3.191539	0.004049	0.713653
-21.248249	-1.842148	3.201536	0.003898	0.713916
-21.339921	-1.800691	3.211533	0.003914	0.713967
-20.862504	-1.886342	3.221530	0.003825	0.713967
-20.735645	-1.867614	3.231526	0.003801	0.714050
-20.165025	-1.856462	3.241523	0.003694	0.714275
-20.089080	-1.870625	3.251520	0.003680	0.714275
-20.128290	-1.863958	3.261517	0.003686	0.714275
-19.514126	-1.866664	3.271514	0.003572	0.714488
-19.135057	-1.873981	3.281510	0.003500	0.714608
-19.067158	-1.887026	3.291507	0.003487	0.714607
-19.111023	-1.882875	3.301504	0.003495	0.714601
-18.553135	-1.838133	3.311501	0.003391	0.714888
-18.310973	-1.873835	3.321498	0.003345	0.714904
-18.377579	-1.861735	3.331494	0.003357	0.714905
-18.043447	-1.841511	3.341491	0.003294	0.715064
-17.223520	-1.906038	3.351488	0.003141	0.715227
-17.656129	-1.828815	3.361485	0.003221	0.715228
-17.317722	-1.889261	3.371482	0.003158	0.715229
-16.686569	-1.859996	3.381478	0.003040	0.715511
-16.404411	-1.892250	3.391475	0.002987	0.715548
-16.372871	-1.900196	3.401472	0.002980	0.715544
-16.362904	-1.876471	3.411469	0.002978	0.715595
-15.474469	-1.889882	3.421466	0.002812	0.715883
-15.177640	-1.942918	3.431462	0.002756	0.715884
-15.482855	-1.889852	3.441459	0.002812	0.715882
-15.128644	-1.921205	3.451456	0.002746	0.715946
-14.719325	-1.899808	3.461453	0.002669	0.716134
-14.214385	-1.992401	3.471450	0.002575	0.716130
-14.856510	-1.877544	3.481446	0.002694	0.716132
-14.166383	-1.896790	3.491443	0.002565	0.716338
-13.882114	-1.893519	3.501440	0.002511	0.716446
-13.885089	-1.893070	3.511437	0.002511	0.716446
-13.616828	-1.902492	3.521434	0.002461	0.716523
-12.866211	-1.919340	3.531430	0.002321	0.716756
-12.703370	-1.948821	3.541427	0.002290	0.716756
-12.900554	-1.912672	3.551424	0.002326	0.716759
-12.482953	-1.876519	3.561421	0.002248	0.716978
-11.791216	-1.947315	3.571418	0.002119	0.717083
-11.866479	-1.933041	3.581414	0.002132	0.717086
-11.584586	-1.983570	3.591411	0.002079	0.717086
-11.365880	-1.885297	3.601408	0.002038	0.717358
-10.944460	-1.950797	3.611405	0.001959	0.717378
-11.078145	-1.926314	3.621402	0.001983	0.717380
-10.834207	-1.902886	3.631398	0.001937	0.717514
-9.922919	-1.968498	3.641395	0.001767	0.717706
-10.281605	-1.907656	3.651392	0.001834	0.717701
-10.172493	-1.928712	3.661389	0.001813	0.717698
-9.280093	-1.945759	3.671386	0.001646	0.717980
-9.273468	-1.928663	3.681382	0.001644	0.718017
-9.008127	-1.974698	3.691379	0.001595	0.718020
-9.358452	-1.878674	3.701376	0.001659	0.718087
-8.137143	-1.960986	3.711373	0.001431	0.718355
-8.115078	-1.967014	3.721370	0.001427	0.718352
-8.113145	-1.965458	3.731366	0.001426	0.718357
-7.897583	-1.949861	3.741363	0.001385	0.718464
-7.268825	-1.973718	3.751360	0.001268	0.718639
-7.343809	-1.960323	3.761357	0.001281	0.718640
-7.357534	-1.956731	3.771354	0.001283	0.718643
-7.082718	-1.895067	3.781350	0.001231	0.718863
-6.521177	-1.943187	3.791347	0.001126	0.718966
-6.594953	-1.931592	3.801344	0.001140	0.718964
-6.427611	-1.903594	3.811341	0.001108	0.719079
-5.512617	-1.972597	3.821338	0.000937	0.719265
-5.578405	-1.959017	3.831334	0.000949	0.719270
-5.607321	-1.955492	3.841331	0.000954	0.719267
-5.071990	-1.917523	3.851328	0.000854	0.719531
-4.467074	-1.991631	3.861325	0.000741	0.719598
-4.652838	-1.957873	3.871322	0.000775	0.719601
-4.542025	-1.966029	3.881318	0.000753	0.719624
-3.813963	-1.956044	3.891315	0.000617	0.719901
-3.818705	-1.955318	3.901312	0.000618	0.719901
-3.631618	-1.991610	3.911309	0.000582	0.719896
-3.546506	-1.943053	3.921306	0.000566	0.720023
-2.603960	-2.008884	3.931302	0.000390	0.720225
-2.869016	-1.962593	3.941299	0.000439	0.720224
-2.801066	-1.975527	3.951296	0.000426	0.720223
-2.614513	-1.880256	3.961293	0.000391	0.720477
-2.281967	-1.907673	3.971290	0.000328	0.720540
-2.016515	-1.954506	3.981286	0.000278	0.720542
-1.752306	-1.914986	3.991283	0.000229	0.720714
-1.458311	-1.881860	4.001280	0.000173	0.720883
-1.469528	-1.882284	4.011277	0.000175	0.720879
-1.399361	-1.856441	4.021274	0.000161	0.720955
-1.114519	-1.822053	4.031270	0.000108	0.721124
-1.278171	-1.792750	4.041267	0.000138	0.721125
-1.149110	-1.710010	4.051264	0.000113	0.721334
-1.154496	-1.657053	4.061261	0.000114	0.721437
-0.788292	-1.662939	4.071258	0.000045	0.721554
-0.762913	-1.569945	4.081254	0.000040	0.721747
-0.755651	-1.534404	4.091251	0.000038	0.721820
-0.762207	-1.404134	4.101248	0.000038	0.722075
-0.526577	-1.402951	4.111245	-0.000006	0.722160
-0.765919	-1.254498	4.121242	0.000038	0.722369
-0.608972	-1.183705	4.131238	0.000008	0.722564
-0.574242	-1.123661	4.141235	0.000001	0.722695
-0.506825	-0.976922	4.151232	-0.000012	0.723007
-0.545772	-0.883794	4.161229	-0.000005	0.723177
-0.526951	-0.785664	4.171226	-0.000009	0.723377
-0.429678	-0.671286	4.181222	-0.000028	0.723636
-0.213423	-0.586143	4.191219	-0.000069	0.723879
-0.501700	-0.419671	4.201216	-0.000016	0.724106
-0.281993	-0.334740	4.211213	-0.000057	0.724350
-0.346057	-0.183634	4.221210	-0.000046	0.724624
-0.061356	-0.098319	4.231206	-0.000099	0.724891
-0.086342	0.062760	4.241203	-0.000095	0.725198
0.000000	0.201196	4.251200	-0.000112	0.725500

0.036947	0.819530	4.256205	-0.000120	0.726721
0.104102	2.083908	4.261210	-0.000133	0.729208
0.510489	3.880706	4.266214	-0.000210	0.732834
0.585606	6.289280	4.271219	-0.000226	0.737506
0.720185	9.192072	4.276224	-0.000253	0.743113
1.006865	12.559255	4.281229	-0.000309	0.749608
1.081963	16.401022	4.286234	-0.000326	0.756866
1.484286	20.594872	4.291238	-0.000404	0.764816
1.998291	25.180448	4.296243	-0.000503	0.773440
2.191076	30.175664	4.301248	-0.000542	0.782607
2.512854	35.508889	4.306253	-0.000606	0.792314
3.276043	41.063170	4.311258	-0.000752	0.802432
3.643240	47.013752	4.316262	-0.000824	0.812993
3.873634	53.254673	4.321267	-0.000871	0.823877
4.569629	59.697651	4.326272	-0.001005	0.835101
5.166978	66.375102	4.331277	-0.001121	0.846540
5.839827	73.266303	4.336282	-0.001251	0.858201
6.237857	80.415958	4.341286	-0.001330	0.870048
6.802543	87.711075	4.346291	-0.001440	0.882017
7.249215	95.208488	4.351296	-0.001529	0.894113
7.988695	102.809011	4.356301	-0.001672	0.906288
8.736557	110.550230	4.361306	-0.001816	0.918522
9.560040	118.398510	4.366310	-0.001975	0.930777
10.110225	126.408501	4.371315	-0.002083	0.943044
10.701013	134.521762	4.376320	-0.002198	0.955317
12.749386	142.480397	4.381325	-0.002585	0.967580
13.486009	150.769778	4.386330	-0.002728	0.979836
14.095950	159.168866	4.391334	-0.002847	0.992066
14.708111	167.595039	4.396339	-0.002967	1.004185
15.417597	176.047129	4.401344	-0.003105	1.016219
15.898146	184.587113	4.406349	-0.003200	1.028177
16.461181	193.134247	4.411354	-0.003311	1.040028
17.236326	201.683807	4.416358	-0.003461	1.051797
17.617251	210.322515	4.421363	-0.003538	1.063464
18.746327	218.868738	4.426368	-0.003754	1.075052
19.786409	227.433215	4.431373	-0.003953	1.086519
20.099372	236.132679	4.436378	-0.004018	1.097879
20.852522	244.758552	4.441382	-0.004164	1.109125
21.373030	253.426421	4.446387	-0.004266	1.120261
22.054045	262.049672	4.451392	-0.004399	1.131265
22.531562	270.726991	4.456397	-0.004494	1.142186
22.924341	279.423882	4.461402	-0.004573	1.153010
23.583924	288.035329	4.466406	-0.004702	1.163685
24.376694	296.614054	4.471411	-0.004855	1.174250
25.285235	305.164185	4.476416	-0.005030	1.184710
25.762918	313.807128	4.481421	-0.005125	1.195101
26.381274	322.375870	4.486426	-0.005246	1.205343
26.641719	331.018203	4.491430	-0.005300	1.215513
27.191443	339.579244	4.496435	-0.005408	1.225562
27.678698	348.158675	4.501440	-0.005505	1.235537
28.244532	356.685484	4.506445	-0.005616	1.245388
29.222536	365.138172	4.511450	-0.005804	1.255156
30.140521	373.601520	4.516454	-0.005981	1.264849
30.804239	382.115275	4.521459	-0.006110	1.274476
30.929821	390.673500	4.526464	-0.006139	1.283979
31.716774	399.138210	4.531469	-0.006292	1.293432
32.097047	407.630830	4.536474	-0.006368	1.302772
32.539619	416.207836	4.541478	-0.006456	1.312148
33.206148	424.652083	4.546483	-0.006586	1.321355
34.139930	432.995014	4.551488	-0.006766	1.330438
34.281143	441.479163	4.556493	-0.006798	1.339468
34.626496	449.889747	4.561498	-0.006868	1.348396
35.294497	458.260517	4.566502	-0.006998	1.357279
35.792525	466.631610	4.571507	-0.007097	1.366076
36.432074	474.993082	4.576512	-0.007221	1.374830
37.004616	483.361523	4.581517	-0.007334	1.383525
37.422075	491.755627	4.586522	-0.007417	1.392165
37.584156	500.152652	4.591526	-0.007453	1.400711
38.154890	508.478046	4.596531	-0.007565	1.409202
38.739227	516.798117	4.601536	-0.007679	1.417638
39.232104	525.128790	4.606541	-0.007777	1.426020
39.557901	533.480253	4.611546	-0.007843	1.434346
39.921111	541.804048	4.616550	-0.007916	1.442602
40.517370	550.089642	4.621555	-0.008033	1.450812
40.750263	558.422837	4.626560	-0.008082	1.458963
41.380811	566.698788	4.631565	-0.008205	1.467077
41.933433	575.028733	4.636570	-0.008314	1.475186
42.420722	583.296056	4.641574	-0.008410	1.483180
42.832207	591.573611	4.646579	-0.008492	1.491128
43.227266	599.846431	4.651584	-0.008572	1.499028
44.180566	608.043148	4.656589	-0.008755	1.506900
44.523865	616.348210	4.661594	-0.008824	1.514739
45.041309	624.595971	4.666598	-0.008926	1.522510
45.680383	632.833932	4.671603	-0.009051	1.530252
45.959658	641.126453	4.676608	-0.009109	1.537950
46.697336	649.328679	4.681613	-0.009252	1.545595
47.162807	657.610755	4.686618	-0.009344	1.553235
47.367891	665.877282	4.691622	-0.009388	1.560785
47.528806	674.145136	4.696627	-0.009423	1.568294
48.133379	682.343237	4.701632	-0.009541	1.575768
48.567519	690.573084	4.706637	-0.009628	1.583211
48.879332	698.816863	4.711642	-0.009692	1.590613
49.220545	707.053704	4.716646	-0.009761	1.597979
49.624118	715.260955	4.721651	-0.009841	1.605294
50.049476	723.472805	4.726656	-0.009926	1.612582
50.528269	731.675937	4.731661	-0.010021	1.619838
50.786669	739.903460	4.736666	-0.010075	1.627052
51.146019	748.177291	4.741670	-0.010147	1.634287
51.428861	756.369643	4.746675	-0.010206	1.641410
51.713218	764.558453	4.751680	-0.010264	1.648499
52.391024	772.716594	4.756685	-0.010396	1.655585
52.733636	780.889357	4.761690	-0.010465	1.662608
53.189980	789.072040	4.766694	-0.010556	1.669625
53.461065	797.291711	4.771699	-0.010612	1.676618
53.685476	805.474003	4.776704	-0.010659	1.683545
54.281288	813.626681	4.781709	-0.010776	1.690468
54.860023	821.781720	4.786714	-0.010889	1.697362
55.246272	829.964868	4.791718	-0.010967	1.704226
55.766381	838.148096	4.796723	-0.011069	1.711080
56.245746	846.317916	4.801728	-0.011164	1.717890
56.553215	854.490102	4.806733	-0.011227	1.724652
57.038396	862.656322	4.811738	-0.011323	1.731407
57.580129	870.821761	4.816742	-0.011429	1.738141
58.082244	878.971800	4.821747	-0.011528	1.744831
58.113601	887.193307	4.826752	-0.011539	1.751495
58.486401	895.369600	4.831757	-0.011614	1.758139
58.710103	903.517027	4.836762	-0.011662	1.764716
59.182687	911.663166	4.841766	-0.011755	1.771299
59.376601	919.857601	4.846771	-0.011797	1.777862
59.766888	927.983756	4.851776	-0.011875	1.784370
60.156113	936.169774	4.856781	-0.011953	1.790901
60.584496	944.328496	4.861786	-0.012039	1.797392
60.780618	952.472171	4.866790	-0.012081	1.803820
61.171754	960.591209	4.871795	-0.012159	1.810229
61.434173	968.756697	4.876800	-0.012213	1.816635
61.766729	976.889222	4.881805	-0.012281	1.823002
62.207774	985.010012	4.886810	-0.012369	1.829351
62.610131	993.141930	4.891814	-0.012449	1.835681
62.940944	1001.284070	4.896819	-0.012516	1.841989
63.012204	1009.446596	4.901824	-0.012535	1.848261
63.784766	1017.553199	4.906829	-0.012684	1.854551
63.965866	1025.696096	4.911834	-0.012724	1.860777
64.382364	1033.822047	4.916838	-0.012807	1.866998
64.583263	1042.011927	4.921843	-0.012850	1.873221
65.158307	1050.079998	4.926848	-0.012962	1.879374
65.512784	1058.199489	4.931853	-0.013034	1.885521
65.825700	1066.333158	4.936858	-0.013098	1.891654
65.927271	1074.506999	4.941862	-0.013122	1.897772
66.229303	1082.617733	4.946867	-0.013184	1.903847
66.777847	1090.710378	4.951872	-0.013292	1.909917
67.569436	1098.788920	4.956877	-0.013445	1.915983
67.650062	1106.943751	4.961882	-0.013465	1.922008
68.123493	1115.057562	4.966886	-0.013559	1.928027
68.723595	1123.170830	4.971891	-0.013676	1.934041
68.896374	1131.310654	4.976896	-0.013714	1.940008
69.454042	1139.408863	4.981901	-0.013823	1.945969
69.984965	1147.554288	4.986906	-0.013928	1.951943
70.261320	1155.697660	4.991910	-0.013985	1.957869
70.609657	1163.790220	4.996915	-0.014055	1.963749
70.664770	1171.923380	5.001920	-0.014071	1.969608
71.078841	1180.043147	5.006925	-0.014153	1.975479
71.448650	1188.117778	5.011930	-0.014228	1.981296
71.907202	1196.204789	5.016934	-0.014319	1.987113
72.262483	1204.339832	5.021939	-0.014390	1.992937
72.655266	1212.428170	5.026944	-0.014469	1.998714
72.820982	1220.563320	5.031949	-0.014505	2.004484
73.167503	1228.650504	5.036954	-0.014575	2.010222
73.533668	1236.765313	5.041958	-0.014649	2.015966
73.900473	1244.859785	5.046963	-0.014723	2.021679
74.158322	1252.970514	5.051968	-0.014777	2.027375
74.676168	1261.091099	5.056973	-0.014879	2.033090
75.151917	1269.165832	5.061978	-0.014973	2.038751
75.523247	1277.249668	5.066982	-0.015047	2.044393
75.851902	1285.364450	5.071987	-0.015114	2.050036
76.117448	1293.478471	5.076992	-0.015169	2.055657
76.552033	1301.568141	5.081997	-0.015255	2.061263
76.603166	1309.697022	5.087002	-0.015271	2.066841
76.960726	1317.803891	5.092006	-0.015343	2.072421
77.376191	1325.888253	5.097011	-0.015425	2.077975
77.429865	1333.987495	5.102016	-0.015441	2.083489
77.763699	1342.095415	5.107021	-0.015509	2.089022
78.150120	1350.182357	5.112026	-0.015586	2.094531
78.480868	1358.270023	5.117030	-0.015653	2.100020
79.068607	1366.311498	5.122035	-0.015768	2.105490
79.308769	1374.454874	5.127040	-0.015818	2.110979
79.529202	1382.609891	5.132045	-0.015865	2.116460
79.957066	1390.643741	5.137050	-0.015950	2.121866
80.217194	1398.731959	5.142054	-0.016004	2.127278
80.405090	1406.847612	5.147059	-0.016045	2.132688
80.668527	1414.926012	5.152064	-0.016099	2.138066
80.998764	1423.004515	5.157069	-0.016166	2.143437
81.223562	1431.095178	5.162074	-0.016214	2.148793
81.311946	1439.226669	5.167078	-0.016236	2.154150
81.574473	1447.299537	5.172083	-0.016290	2.159471
81.768678	1455.354747	5.177088	-0.016332	2.164761
82.245516	1463.434341	5.182093	-0.016426	2.170080
82.638764	1471.526577	5.187098	-0.016505	2.175386
82.835332	1479.615568	5.192102	-0.016547	2.180659
83.178993	1487.679806	5.197107	-0.016616	2.185917
83.551955	1495.763206	5.202112	-0.016691	2.191178
84.098976	1503.843400	5.207117	-0.016799	2.196439
84.268881	1511.912114	5.212122	-0.016836	2.201646
84.474978	1519.993748	5.217126	-0.016880	2.206852
84.986095	1528.062656	5.222131	-0.016980	2.212065
85.297252	1536.130181	5.227136	-0.017044	2.217247
85.524353	1544.229116	5.232141	-0.017092	2.222430
85.860889	1552.290987	5.237146	-0.017160	2.227586
86.179788	1560.393973	5.242150	-0.017225	2.232755
86.615772	1568.461580	5.247155	-0.017311	2.237900
86.444958	1576.575904	5.252160	-0.017285	2.243009
86.901502	1584.626584	5.257165	-0.017376	2.248122
87.269675	1592.701026	5.262170	-0.017450	2.253229
87.509969	1600.795655	5.267174	-0.017500	2.258327
88.097886	1608.840252	5.272179	-0.017615	2.263412
88.277124	1616.925754	5.277184	-0.017654	2.268476
88.623203	1625.092405	5.282189	-0.017724	2.273593
88.747970	1633.149163	5.287194	-0.017753	2.278612
89.163188	1641.171328	5.292198	-0.017835	2.283623
89.572098	1649.219861	5.297203	-0.017917	2.288638
89.866205	1657.291273	5.302208	-0.017977	2.293647
90.195679	1665.363254	5.307213	-0.018044	2.298648
90.561454	1673.407908	5.312218	-0.018118	2.303625
90.926424	1681.474665	5.317222	-0.018191	2.308604
91.403097	1689.564232	5.322227	-0.018286	2.313595
91.593575	1697.626820	5.327232	-0.018326	2.318536
92.043729	1705.676938	5.332237	-0.018416	2.323480
92.255156	1713.757282	5.337242	-0.018461	2.328411
92.636232	1721.837228	5.342246	-0.018537	2.333346
92.884652	1729.922912	5.347251	-0.018589	2.338264
92.951045	1738.004995	5.352256	-0.018607	2.343153
93.242509	1746.075843	5.357261	-0.018667	2.348044
93.552167	1754.174770	5.362266	-0.018730	2.352944
93.961223	1762.209711	5.367270	-0.018811	2.357802
94.198115	1770.284487	5.372275	-0.018861	2.362661
94.522254	1778.327196	5.377280	-0.018927	2.367497
94.893602	1786.411383	5.382285	-0.019002	2.372352
95.166046	1794.461404	5.387290	-0.019058	2.377168
95.265783	1802.551381	5.392294	-0.019082	2.381985
95.771284	1810.581849	5.397299	-0.019181	2.386789
95.736710	1818.699247	5.402304	-0.019181	2.391592
96.038533	1826.779816	5.407309	-0.019242	2.396390
96.444651	1834.784172	5.412314	-0.019323	2.401142
96.566353	1842.850245	5.417318	-0.019352	2.405898
96.782184	1850.952310	5.422323	-0.019397	2.410673
97.268678	1858.982666	5.427328	-0.019493	2.415418
97.664956	1867.034426	5.432333	-0.019573	2.420159
97.768764	1875.111799	5.437338	-0.019597	2.424883
98.267005	1883.160093	5.442342	-0.019696	2.429611
99.199465	1891.239621	5.447347	-0.019875	2.434381
99.215936	1899.292413	5.452352	-0.019883	2.439057
99.570129	1907.350749	5.457357	-0.019955	2.443752
100.240056	1915.360896	5.462362	-0.020085	2.448434
100.611882	1923.430272	5.467366	-0.020160	2.453119
100.798285	1931.519274	5.472371	-0.020200	2.457792
100.971740	1939.584182	5.477376	-0.020238	2.462441
101.455513	1947.628541	5.482381	-0.020333	2.467093
101.601950	1955.712219	5.487386	-0.020366	2.471733
102.012972	1963.760056	5.492390	-0.020448	2.476364
102.371923	1971.819321	5.497395	-0.020521	2.480989
102.746530	1979.848204	5.502400	-0.020596	2.485589
102.806836	1987.944233	5.507405	-0.020613	2.490195
103.163501	1996.009221	5.512410	-0.020684	2.494797
103.392148	2004.063121	5.517414	-0.020733	2.499375
103.787196	2012.101341	5.522419	-0.020812	2.503948
104.121148	2020.166264	5.527424	-0.020879	2.508523
104.556406	2028.261946	5.532429	-0.020966	2.513114
104.769299	2036.307070	5.537434	-0.021011	2.517652
104.849889	2044.371296	5.542438	-0.021031	2.522183
105.364407	2052.403983	5.547443	-0.021133	2.526719
105.445359	2060.466093	5.552448	-0.021153	2.531233
105.633406	2068.555012	5.557453	-0.021194	2.535761
105.844893	2076.601403	5.562458	-0.021239	2.540259
106.079186	2084.644122	5.567462	-0.021288	2.544749
106.208621	2092.723817	5.572467	-0.021317	2.549243
106.323692	2100.805589	5.577472	-0.021344	2.553730
106.649196	2108.832623	5.582477	-0.021411	2.558194
106.994540	2116.857513	5.587482	-0.021480	2.562650
107.028029	2124.917003	5.592486	-0.021492	2.567095
107.273392	2132.996699	5.597491	-0.021543	2.571559
107.527715	2141.042539	5.602496	-0.021596	2.575997
107.729245	2149.115610	5.607501	-0.021639	2.580438
108.106970	2157.121812	5.612506	-0.021715	2.584847
108.384716	2165.163604	5.617510	-0.021772	2.589261
108.679235	2173.420514	5.622515	-0.021833	2.593786
108.988406	2181.409655	5.627520	-0.021896	2.598159
109.390729	2189.390481	5.632525	-0.021976	2.602525
109.576757	2197.405289	5.637530	-0.022016	2.606889
109.793448	2205.450588	5.642534	-0.022062	2.611263
110.180666	2213.502780	5.647539	-0.022140	2.615645
110.395048	2221.523036	5.652544	-0.022185	2.619991
110.556817	2229.567607	5.657549	-0.022221	2.624339
110.756717	2237.627298	5.662554	-0.022263	2.628691
111.125643	2245.695894	5.667558	-0.022337	2.633052
111.146238	2253.768016	5.672563	-0.022347	2.637384
111.168509	2261.798974	5.677568	-0.022356	2.641687
111.777763	2269.801042	5.682573	-0.022475	2.646006
111.894517	2277.858808	5.687578	-0.022503	2.650315
112.053514	2285.935441	5.692582	-0.022538	2.654631
112.328095	2293.979482	5.697587	-0.022594	2.658929
112.488437	2302.008895	5.702592	-0.022630	2.663205
112.860411	2310.075012	5.707597	-0.022704	2.667508
113.643167	2318.087296	5.712602	-0.022856	2.671801
113.980272	2326.157018	5.717606	-0.022924	2.676089
114.353977	2334.181586	5.722611	-0.022999	2.680349
114.535383	2342.192032	5.727616	-0.023038	2.684582
114.796365	2350.270345	5.732621	-0.023092	2.688849
115.059688	2358.331036	5.737626	-0.023147	2.693100
115.369860	2366.370983	5.742630	-0.023210	2.697337
115.791957	2374.401944	5.747635	-0.023294	2.701569
116.061390	2382.434803	5.752640	-0.023350	2.705786
116.337797	2390.503464	5.757645	-0.023407	2.710015
116.483123	2398.579008	5.762650	-0.023439	2.714233
116.957533	2406.588854	5.767654	-0.023533	2.718431
117.167023	2414.640566	5.772659	-0.023578	2.722628
117.479556	2422.683522	5.777664	-0.023641	2.726820
117.747662	2430.762422	5.782669	-0.023697	2.731021
117.882496	2438.841355	5.787674	-0.023727	2.735208
117.832473	2446.868745	5.792678	-0.023724	2.739350
118.369905	2454.900560	5.797683	-0.023829	2.743524
118.511902	2462.950369	5.802688	-0.023861	2.747677
118.739934	2471.052749	5.807693	-0.023909	2.751856
118.858564	2479.154289	5.812698	-0.023937	2.756021
119.079161	2487.142780	5.817702	-0.023983	2.760128
119.444225	2495.136118	5.822707	-0.024057	2.764241
119.421760	2503.179029	5.827712	-0.024058	2.768349
119.986372	2511.211143	5.832717	-0.024169	2.772481
120.216906	2519.260846	5.837722	-0.024217	2.776595
120.110734	2527.334854	5.842726	-0.024203	2.780696
120.496259	2535.346897	5.847731	-0.024280	2.784788
120.704507	2543.382924	5.852736	-0.024324	2.788876
121.045195	2551.443267	5.857741	-0.024393	2.792978
121.241396	2559.481727	5.862746	-0.024435	2.797055
121.775096	2567.460843	5.867750	-0.024540	2.801115
122.220768	2575.504137	5.872755	-0.024628	2.805196
122.198186	2583.565567	5.877760	-0.024630	2.809254
122.334933	2591.659474	5.882765	-0.024661	2.813331
122.864072	2599.650449	5.887770	-0.024765	2.817373
123.239960	2607.691336	5.892774	-0.024840	2.821425
123.661311	2615.744416	5.897779	-0.024924	2.825480
123.423411	2623.811484	5.902784	-0.024885	2.829499
123.900235	2631.884132	5.907789	-0.024980	2.833555
124.125560	2639.910120	5.912794	-0.025027	2.837568
124.156237	2647.964702	5.917798	-0.025038	2.841579
124.403955	2655.977776	5.922803	-0.025090	2.845575
124.652155	2663.999058	5.927808	-0.025142	2.849570
124.991588	2672.069966	5.932813	-0.025210	2.853589
125.381397	2680.081740	5.937818	-0.025288	2.857576
125.399694	2688.136668	5.942822	-0.025297	2.861558
125.756931	2696.169142	5.947827	-0.025369	2.865542
126.115616	2704.181140	5.952832	-0.025442	2.869510
126.432257	2712.259296	5.957837	-0.025506	2.873503
126.445951	2720.330639	5.962842	-0.025514	2.877471
126.638510	2728.332047	5.967846	-0.025555	2.881408
127.110528	2736.351599	5.972851	-0.025649	2.885364
127.198849	2744.396406	5.977856	-0.025671	2.889306
127.337936	2752.480494	5.982861	-0.025702	2.893265
127.756137	2760.501893	5.987866	-0.025785	2.897203
127.865230	2768.551359	5.992870	-0.025811	2.901132
128.052388	2776.580071	5.997875	-0.025852	2.905050
128.220639	2784.632743	6.002880	-0.025888	2.908974
128.662798	2792.736369	6.007885	-0.025976	2.912931
128.968275	2800.767045	6.012890	-0.026039	2.916841
129.232394	2808.760934	6.017894	-0.026093	2.920725
129.339895	2816.778894	6.022899	-0.026119	2.924607
129.418436	2824.818505	6.027904	-0.026139	2.928493
129.791271	2832.848381	6.032909	-0.026214	2.932384
130.191680	2840.904294	6.037914	-0.026294	2.936285
130.511487	2848.897404	6.042918	-0.026359	2.940145
130.711839	2856.959053	6.047923	-0.026402	2.944028
130.941108	2864.984682	6.052928	-0.026450	2.947889
131.393638	2873.022249	6.057933	-0.026540	2.951762
131.426620	2881.121805	6.062938	-0.026551	2.955639
131.542460	2889.103420	6.067942	-0.026578	2.959458
132.085258	2897.129358	6.072947	-0.026685	2.963315
132.371758	2905.143747	6.077952	-0.026744	2.967149
132.556288	2913.219638	6.082957	-0.026783	2.971001
132.740642	2921.289704	6.087962	-0.026823	2.974846
132.869153	2929.307828	6.092966	-0.026853	2.978658
133.113884	2937.339725	6.097971	-0.026904	2.982478
133.287369	2945.367862	6.102976	-0.026942	2.986287
133.730486	2953.396206	6.107981	-0.027030	2.990106
133.965471	2961.484249	6.112986	-0.027079	2.993937
134.331908	2969.470830	6.117990	-0.027153	2.997721
134.753168	2977.475178	6.122995	-0.027236	3.001512
134.713466	2985.525201	6.128000	-0.027235	3.005297
134.923875	2993.569007	6.133005	-0.027279	3.009087
135.289962	3001.629353	6.138010	-0.027353	3.012887
135.647535	3009.629638	6.143014	-0.027425	3.016653
136.002463	3017.667091	6.148019	-0.027496	3.020433
136.041459	3025.706376	6.153024	-0.027509	3.024192
136.342142	3033.755171	6.158029	-0.027571	3.027965
136.411119	3041.821535	6.163034	-0.027589	3.031729
136.641632	3049.862404	6.168038	-0.027637	3.035485
136.832993	3057.880478	6.173043	-0.027679	3.039224
137.031834	3065.902378	6.178048	-0.027721	3.042960
137.217061	3073.955180	6.183053	-0.027761	3.046705
137.598338	3081.975532	6.188058	-0.027838	3.050440
137.981409	3090.015184	6.193062	-0.027914	3.054179
138.262008	3098.046361	6.198067	-0.027972	3.057905
138.367047	3106.082479	6.203072	-0.027997	3.061620
138.805871	3114.094942	6.208077	-0.028084	3.065335
139.125204	3122.126172	6.213082	-0.028149	3.069049
139.410797	3130.227789	6.218086	-0.028208	3.072790
139.893314	3138.264320	6.223091	-0.028303	3.076504
139.752012	3146.270011	6.228096	-0.028282	3.080172
140.122839	3154.259853	6.233101	-0.028357	3.083851
140.423416	3162.282917	6.238106	-0.028418	3.087538
140.617024	3170.332682	6.243110	-0.028460	3.091227
140.808388	3178.413603	6.248115	-0.028501	3.094926
140.875384	3186.420925	6.253120	-0.028519	3.098582
141.204546	3194.439542	6.258125	-0.028586	3.102250
141.449135	3202.485909	6.263130	-0.028637	3.105923
141.548054	3210.511823	6.268134	-0.028661	3.109576
141.984777	3218.563064	6.273139	-0.028748	3.113250
142.521319	3226.545904	6.278144	-0.028853	3.116894
142.493580	3234.632391	6.283149	-0.028853	3.120556
142.712027	3242.636272	6.288154	-0.028899	3.124186
143.133297	3250.645400	6.293158	-0.028983	3.127824
143.325136	3258.740042	6.298163	-0.029025	3.131486
143.454396	3266.757576	6.303168	-0.029054	3.135106
143.597374	3274.800443	6.308173	-0.029086	3.138733
143.691886	3282.831757	6.313178	-0.029109	3.142350
143.676202	3290.872055	6.318182	-0.029112	3.145961
144.022730	3298.902859	6.323187	-0.029182	3.149580
144.097754	3306.944502	6.328192	-0.029201	3.153187
144.560320	3314.981357	6.333197	-0.029293	3.156805
144.817022	3322.961069	6.338202	-0.029346	3.160385
145.209986	3330.966111	6.343206	-0.029425	3.163977
145.439041	3339.008236	6.348211	-0.029473	3.167575
145.557828	3347.061174	6.353216	-0.029501	3.171169
145.965644	3355.096834	6.358221	-0.029582	3.174763
146.247947	3363.131413	6.363226	-0.029640	3.178347
146.261061	3371.158873	6.368230	-0.029648	3.181913
146.504565	3379.211989	6.373235	-0.029699	3.185496
146.757321	3387.222656	6.378240	-0.029751	3.189056
146.969316	3395.277356	6.383245	-0.029796	3.192630
147.136872	3403.322820	6.388250	-0.029833	3.196194
147.100001	3411.342333	6.393254	-0.029832	3.199734
147.606515	3419.330470	6.398259	-0.029931	3.203279
147.603656	3427.378090	6.403264	-0.029936	3.206825
147.933657	3435.400320	6.408269	-0.030003	3.210370
148.199539	3443.463214	6.413274	-0.030058	3.213926
148.431765	3451.475041	6.418278	-0.030107	3.217454
148.772856	3459.532555	6.423283	-0.030176	3.221003
149.049368	3467.507522	6.428288	-0.030233	3.224509
149.441746	3475.552551	6.433293	-0.030311	3.228046
149.546222	3483.626340	6.438298	-0.030336	3.231581
149.821443	3491.670949	6.443302	-0.030393	3.235106
149.923863	3499.706887	6.448307	-0.030418	3.238616
150.185749	3507.706702	6.453312	-0.030472	3.242113
150.534526	3515.690025	6.458317	-0.030542	3.245602
150.813006	3523.701541	6.463322	-0.030600	3.249097
150.987004	3531.773888	6.468326	-0.030638	3.252611
151.200163	3539.844254	6.473331	-0.030683	3.256121
151.625129	3547.800222	6.478336	-0.030767	3.259587
151.981358	3555.825276	6.483341	-0.030839	3.263075
152.035794	3563.895352	6.488346	-0.030855	3.266568
152.135067	3571.913617	6.493350	-0.030879	3.270036
152.451717	3579.993042	6.498355	-0.030943	3.273536
152.492236	3588.004917	6.503360	-0.030956	3.276991
152.541762	3596.048396	6.508365	-0.030971	3.280457
153.049983	3604.020449	6.513370	-0.031071	3.283907
153.191315	3612.058233	6.518374	-0.031103	3.287367
153.306710	3620.122175	6.523379	-0.031130	3.290833
153.633200	3628.133471	6.528384	-0.031196	3.294281
154.145933	3636.163608	6.533389	-0.031297	3.297741
153.997118	3644.216359	6.538394	-0.031275	3.301182
154.442150	3652.191557	6.543398	-0.031363	3.304608
154.662155	3660.270637	6.548403	-0.031410	3.308067
154.647360	3668.322773	6.553408	-0.031412	3.311501
155.117207	3676.349087	6.558413	-0.031505	3.314939
155.628738	3684.336990	6.563418	-0.031606	3.318359
155.657398	3692.346637	6.568422	-0.031617	3.321767
155.812952	3700.355557	6.573427	-0.031651	3.325175
156.060050	3708.377242	6.578432	-0.031703	3.328588
156.297535	3716.447180	6.583437	-0.031752	3.332019
156.391244	3724.505686	6.588442	-0.031775	3.335435
156.743646	3732.482734	6.593446	-0.031846	3.338823
157.012545	3740.507114	6.598451	-0.031902	3.342224
157.217887	3748.520176	6.603456	-0.031946	3.345615
157.354562	3756.563720	6.608461	-0.031977	3.349013
157.641139	3764.630705	6.613466	-0.032036	3.352422
157.818022	3772.687320	6.618470	-0.032074	3.355820
158.183218	3780.657971	6.623475	-0.032147	3.359185
158.138646	3788.688374	6.628480	-0.032145	3.362557
158.624701	3796.713326	6.633485	-0.032241	3.365942
158.846691	3804.734170	6.638490	-0.032287	3.369312
159.118516	3812.790976	6.643494	-0.032343	3.372696
159.402057	3820.875918	6.648499	-0.032402	3.376089
159.104618	3828.865297	6.653504	-0.032352	3.379418
159.544152	3836.880733	6.658509	-0.032439	3.382780
159.921114	3844.914146	6.663514	-0.032515	3.386144
160.048081	3852.913116	6.668518	-0.032544	3.389482
160.075315	3861.060493	6.673523	-0.032555	3.392875
160.326608	3869.055272	6.678528	-0.032607	3.396208
160.801279	3877.035552	6.683533	-0.032701	3.399541
160.879648	3885.030689	6.688538	-0.032721	3.402862
160.829150	3893.066275	6.693542	-0.032717	3.406192
161.442692	3901.048416	6.698547	-0.032837	3.409520
161.709893	3909.090050	6.703552	-0.032892	3.412857
161.941913	3917.160735	6.708557	-0.032940	3.416201
162.129214	3925.171297	6.713562	-0.032981	3.419516
162.244366	3933.162366	6.718566	-0.033008	3.422818
162.594530	3941.198714	6.723571	-0.033078	3.426142
162.626364	3949.229718	6.728576	-0.033090	3.429451
163.067263	3957.247922	6.733581	-0.033177	3.432764
163.332299	3965.335567	6.738586	-0.033232	3.436097
163.462615	3973.306007	6.743590	-0.033262	3.439375
163.771854	3981.365516	6.748595	-0.033325	3.442691
163.805984	3989.365318	6.753600	-0.033337	3.445971
163.957935	3997.404431	6.758605	-0.033371	3.449267
164.354617	4005.469749	6.763610	-0.033450	3.452579
164.623176	4013.501341	6.768614	-0.033505	3.455870
164.857807	4021.499835	6.773619	-0.033555	3.459143
164.858173	4029.527850	6.778624	-0.033560	3.462418
165.312930	4037.531763	6.783629	-0.033650	3.465694
165.530570	4045.601501	6.788634	-0.033696	3.468986
165.663636	4053.628138	6.793638	-0.033727	3.472255
165.957786	4061.691143	6.798643	-0.033787	3.475540
166.178454	4069.640774	6.803648	-0.033833	3.478775
166.385574	4077.688323	6.808653	-0.033877	3.482045
166.597645	4085.661434	6.813658	-0.033922	3.485282
166.718480	4093.713275	6.818662	-0.033950	3.488545
167.006813	4101.776588	6.823667	-0.034010	3.491815
166.947735	4109.771157	6.828672	-0.034004	3.495043
167.264020	4117.801097	6.833677	-0.034068	3.498295
167.787921	4125.799281	6.838682	-0.034171	3.501536
167.623062	4133.821339	6.843686	-0.034146	3.504763
168.079373	4141.878706	6.848691	-0.034237	3.508021
168.136051	4149.918702	6.853696	-0.034253	3.511256
168.255018	4157.946579	6.858701	-0.034280	3.514485
168.540727	4165.965986	6.863706	-0.034339	3.517713
168.874635	4173.957273	6.868710	-0.034407	3.520928
169.129459	4181.957389	6.873715	-0.034460	3.524141
169.066992	4190.003155	6.878720	-0.034453	3.527360
169.424439	4198.050886	6.883725	-0.034525	3.530589
169.675689	4206.106391	6.888730	-0.034578	3.533815
169.691500	4214.141804	6.893734	-0.034586	3.537024
169.945287	4222.161095	6.898739	-0.034639	3.540230
170.208630	4230.129838	6.903744	-0.034693	3.543413
170.321020	4238.191736	6.908749	-0.034720	3.546626
170.684040	4246.241462	6.913754	-0.034793	3.549838
170.867423	4254.326997	6.918758	-0.034833	3.553057
171.225370	4262.358969	6.923763	-0.034905	3.556256
171.329885	4270.294324	6.928768	-0.034930	3.559407
171.497319	4278.306976	6.933773	-0.034966	3.562587
171.833470	4286.319933	6.938778	-0.035034	3.565770
172.060227	4294.341162	6.943782	-0.035082	3.568950
172.529321	4302.380300	6.948787	-0.035175	3.572141
172.696654	4310.422067	6.953792	-0.035211	3.575321
172.756804	4318.435369	6.958797	-0.035228	3.578484
172.911694	4326.469493	6.963802	-0.035262	3.581655
173.144959	4334.442464	6.968806	-0.035311	3.584802
173.566802	4342.489848	6.973811	-0.035395	3.587981
173.682973	4350.526944	6.978816	-0.035423	3.591144
173.990087	4358.535152	6.983821	-0.035485	3.594298
174.020400	4366.577609	6.988826	-0.035496	3.597455
174.315504	4374.569925	6.993830	-0.035557	3.600597
174.457727	4382.589067	6.998835	-0.035589	3.603742
174.581765	4390.638929	7.003840	-0.035617	3.606896
174.831894	4398.651789	7.008845	-0.035669	3.610037
175.158915	4406.675884	7.013850	-0.035736	3.613181
175.486332	4414.721499	7.018854	-0.035802	3.616331
175.794188	4422.697183	7.023859	-0.035865	3.619450
175.765123	4430.739665	7.028864	-0.035865	3.622583
175.978639	4438.760053	7.033869	-0.035910	3.625712
176.359493	4446.807880	7.038874	-0.035987	3.628853
176.531232	4454.855751	7.043878	-0.036024	3.631985
176.792723	4462.908434	7.048883	-0.036078	3.635119
176.912029	4470.899165	7.053888	-0.036106	3.638223
177.080295	4478.940124	7.058893	-0.036143	3.641345
177.564216	4486.905004	7.063898	-0.036238	3.644443
177.530421	4494.973839	7.068902	-0.036238	3.647564
177.684435	4502.992268	7.073907	-0.036272	3.650669
177.729969	4511.023403	7.078912	-0.036286	3.653773
177.896901	4519.063633	7.083917	-0.036322	3.656881
178.199279	4527.044074	7.088922	-0.036384	3.659967
178.450498	4535.067284	7.093926	-0.036436	3.663065
178.792073	4543.117255	7.098931	-0.036505	3.666173
178.782210	4551.133775	7.103936	-0.036509	3.669257
179.135746	4559.179739	7.108941	-0.036580	3.672358
179.442822	4567.221147	7.113946	-0.036643	3.675454
179.532205	4575.187167	7.118950	-0.036665	3.678513
180.032794	4583.213925	7.123955	-0.036764	3.681604
180.017303	4591.210202	7.128960	-0.036766	3.684666
180.341377	4599.211850	7.133965	-0.036832	3.687737
180.424399	4607.281165	7.138970	-0.036853	3.690825
180.639217	4615.315087	7.143974	-0.036899	3.693900
180.769576	4623.370352	7.148979	-0.036928	3.696979
180.919569	4631.347597	7.153984	-0.036962	3.700026
181.147962	4639.354234	7.158989	-0.037010	3.703083
181.277955	4647.416649	7.163994	-0.037039	3.706157
181.474848	4655.388727	7.168998	-0.037081	3.709195
181.831993	4663.500010	7.174003	-0.037154	3.712288
182.016566	4671.515071	7.179008	-0.037193	3.715337
182.521062	4679.480847	7.184013	-0.037293	3.718373
182.794477	4687.532417	7.189018	-0.037349	3.721433
182.882819	4695.459157	7.194022	-0.037371	3.724439
182.977409	4703.516508	7.199027	-0.037394	3.727492
183.101532	4711.572034	7.204032	-0.037423	3.730542
183.186453	4719.607780	7.209037	-0.037444	3.733582
183.596431	4727.639518	7.214042	-0.037526	3.736625
183.548369	4735.604200	7.219046	-0.037522	3.739630
184.010497	4743.642652	7.224051	-0.037614	3.742672
184.025738	4751.668562	7.229056	-0.037622	3.745696
184.333493	4759.684389	7.234061	-0.037685	3.748721
184.521440	4767.753306	7.239066	-0.037725	3.751761
184.720008	4775.755904	7.244070	-0.037768	3.754773
184.996168	4783.775200	7.249075	-0.037825	3.757791
185.181972	4791.816624	7.254080	-0.037865	3.760813
185.339290	4799.800546	7.259085	-0.037900	3.763810
185.498726	4807.856639	7.264090	-0.037935	3.766832
185.639242	4815.847010	7.269094	-0.037966	3.769826
185.907922	4823.900306	7.274099	-0.038022	3.772844
186.022560	4831.948622	7.279104	-0.038049	3.775855
186.243388	4839.938458	7.284109	-0.038095	3.778844
186.570596	4847.972679	7.289114	-0.038162	3.781849
186.896550	4855.942313	7.294118	-0.038228	3.784828
187.016121	4864.029651	7.299123	-0.038256	3.787843
186.926986	4872.048680	7.304128	-0.038245	3.790826
187.327818	4880.088534	7.309133	-0.038325	3.793826
187.404029	4888.123913	7.314138	-0.038344	3.796814
187.574439	4896.057495	7.319142	-0.038382	3.799764
187.910207	4904.108793	7.324147	-0.038450	3.802759
188.004103	4912.125187	7.329152	-0.038473	3.805733
188.104676	4920.123905	7.334157	-0.038497	3.808698
188.350610	4928.193838	7.339162	-0.038548	3.811691
188.617111	4936.192199	7.344166	-0.038603	3.814656
188.829078	4944.228792	7.349171	-0.038648	3.817630
188.753165	4952.197874	7.354176	-0.038639	3.820572
189.089669	4960.248380	7.359181	-0.038707	3.823550
189.423231	4968.293628	7.364186	-0.038775	3.826524
189.504267	4976.279180	7.369190	-0.038796	3.829468
189.761725	4984.312627	7.374195	-0.038849	3.832431
190.010118	4992.327455	7.379200	-0.038901	3.835385
190.032888	5000.339239	7.384205	-0.038910	3.838330
190.432172	5008.375951	7.389210	-0.038990	3.841291
190.635485	5016.328781	7.394214	-0.039034	3.844214
190.888312	5024.409323	7.399219	-0.039086	3.847182
190.768270	5032.430077	7.404224	-0.039069	3.850119
191.166700	5040.475023	7.409229	-0.039149	3.853073
191.246594	5048.558465	7.414234	-0.039169	3.856033
191.301237	5056.524834	7.419238	-0.039185	3.858946
191.558005	5064.549407	7.424243	-0.039238	3.861883
192.071718	5072.535336	7.429248	-0.039339	3.864809
192.030105	5080.599803	7.434253	-0.039337	3.867750
192.240788	5088.643827	7.439258	-0.039382	3.870686
192.370471	5096.881095	7.444262	-0.039412	3.873689
192.562809	5104.851972	7.449267	-0.039453	3.876594
192.743114	5112.720496	7.454272	-0.039492	3.879459
193.109713	5120.709554	7.459277	-0.039566	3.882369
193.229178	5128.722271	7.464282	-0.039593	3.885281
193.302276	5136.703930	7.469286	-0.039612	3.888178
193.355473	5144.783945	7.474291	-0.039628	3.891109
193.581537	5152.785954	7.479296	-0.039675	3.894012
193.622995	5160.833086	7.484301	-0.039689	3.896927
193.851540	5168.796167	7.489306	-0.039737	3.899812
194.061708	5176.841377	7.494310	-0.039781	3.902724
194.532417	5184.849738	7.499315	-0.039874	3.905625
194.477535	5192.835269	7.504320	-0.039870	3.908507
194.840470	5200.894287	7.509325	-0.039943	3.911420
195.181029	5208.927699	7.514330	-0.040011	3.914322
195.263172	5216.930173	7.519334	-0.040032	3.917205
195.345097	5224.938596	7.524339	-0.040053	3.920089
195.508585	5232.978339	7.529344	-0.040089	3.922983
195.595768	5240.985375	7.534349	-0.040111	3.925862
195.620340	5249.024978	7.539354	-0.040121	3.928749
195.808393	5257.041402	7.544358	-0.040161	3.931629
196.193954	5265.073062	7.549363	-0.040238	3.934515
196.392540	5273.096585	7.554368	-0.040281	3.937393
196.497651	5281.074886	7.559373	-0.040306	3.940252
196.685024	5289.128292	7.564378	-0.040346	3.943136
197.028242	5297.094379	7.569382	-0.040416	3.945990
197.065193	5305.130390	7.574387	-0.040428	3.948861
197.288540	5313.178903	7.579392	-0.040475	3.951738
197.495832	5321.237669	7.584397	-0.040519	3.954616
197.776616	5329.223481	7.589402	-0.040577	3.957467
198.128076	5337.177566	7.594406	-0.040648	3.960307
198.319180	5345.227718	7.599411	-0.040689	3.963175
198.381046	5353.248717	7.604416	-0.040706	3.966029
198.631394	5361.225225	7.609421	-0.040758	3.968868
199.031984	5369.304181	7.614426	-0.040838	3.971744
199.185797	5377.316376	7.619430	-0.040872	3.974590
199.133166	5385.392561	7.624435	-0.040868	3.977453
199.324283	5393.364395	7.629440	-0.040909	3.980282
199.561320	5401.375116	7.634445	-0.040958	3.983122
199.796805	5409.425275	7.639450	-0.041008	3.985975
199.854520	5417.441861	7.644454	-0.041024	3.988811
200.212877	5425.483882	7.649459	-0.041096	3.991658
200.241030	5433.488618	7.654464	-0.041107	3.994485
200.382128	5441.522195	7.659469	-0.041139	3.997322
200.598257	5449.548382	7.664474	-0.041184	4.000156
200.603813	5457.542057	7.669478	-0.041191	4.002972
200.656479	5465.564078	7.674483	-0.041206	4.005798
200.877383	5473.573567	7.679488	-0.041253	4.008619
201.183669	5481.649814	7.684493	-0.041315	4.011464
201.368520	5489.675129	7.689498	-0.041355	4.014286
201.323588	5497.692373	7.694502	-0.041352	4.017101
201.798011	5505.694919	7.699507	-0.041446	4.019916
201.956297	5513.727897	7.704512	-0.041481	4.022735
202.074509	5521.713074	7.709517	-0.041509	4.025534
202.280604	5529.754444	7.714522	-0.041552	4.028353
202.335097	5537.763498	7.719526	-0.041568	4.031155
202.454323	5545.915601	7.724531	-0.041596	4.034007
202.453464	5553.878467	7.729536	-0.041601	4.036789
202.993296	5561.808438	7.734541	-0.041707	4.039566
203.313563	5569.797335	7.739546	-0.041772	4.042358
203.239735	5577.806853	7.744550	-0.041764	4.045150
203.692466	5585.831876	7.749555	-0.041854	4.047952
203.797755	5593.879082	7.754560	-0.041879	4.050755
203.888683	5601.897508	7.759565	-0.041901	4.053547
204.024305	5609.931319	7.764570	-0.041932	4.056342
204.226441	5617.905950	7.769574	-0.041975	4.059115
204.525498	5625.944189	7.774579	-0.042036	4.061910
204.603065	5633.917996	7.779584	-0.042056	4.064678
204.718883	5641.943451	7.784589	-0.042083	4.067462
204.877873	5649.969999	7.789594	-0.042118	4.070245
204.718349	5658.009618	7.794598	-0.042094	4.073027
205.011599	5666.045428	7.799603	-0.042154	4.075811
205.198345	5674.045980	7.804608	-0.042194	4.078580
205.157992	5682.064745	7.809613	-0.042192	4.081350
205.537634	5690.058678	7.814618	-0.042268	4.084116
205.807903	5698.050758	7.819622	-0.042324	4.086877
206.007505	5706.090997	7.824627	-0.042367	4.089652
205.975931	5714.131347	7.829632	-0.042366	4.092423
206.325574	5722.163182	7.834637	-0.042437	4.095193
206.527968	5730.199062	7.839642	-0.042480	4.097961
206.435306	5738.192824	7.844646	-0.042468	4.100709
206.765172	5746.201136	7.849651	-0.042535	4.103465
206.920883	5754.266193	7.854656	-0.042570	4.106237
207.166092	5762.225076	7.859661	-0.042621	4.108971
207.337377	5770.331494	7.864666	-0.042658	4.111754
207.294962	5778.325770	7.869670	-0.042656	4.114493
207.521007	5786.378233	7.874675	-0.042703	4.117254
207.673859	5794.339467	7.879680	-0.042737	4.119981
207.864650	5802.352121	7.884685	-0.042778	4.122724
208.012867	5810.379991	7.889690	-0.042811	4.125469
208.043780	5818.381920	7.894694	-0.042823	4.128203
208.425565	5826.422127	7.899699	-0.042899	4.130952
208.495702	5834.445283	7.904704	-0.042918	4.133690
208.646679	5842.492866	7.909709	-0.042951	4.136435
208.871644	5850.487289	7.914714	-0.042999	4.139161
209.035532	5858.476419	7.919718	-0.043035	4.141883
209.353109	5866.485621	7.924723	-0.043099	4.144612
209.227406	5874.548035	7.929728	-0.043081	4.147351
209.646970	5882.557993	7.934733	-0.043165	4.150078
209.671908	5890.612927	7.939738	-0.043175	4.152813
209.745877	5898.626387	7.944742	-0.043194	4.155533
210.048016	5906.615156	7.949747	-0.043256	4.158245
210.278506	5914.655050	7.954752	-0.043304	4.160972
210.341118	5922.582468	7.959757	-0.043322	4.163657
210.653520	5930.692977	7.964762	-0.043385	4.166406
210.696972	5938.652752	7.969766	-0.043399	4.169098
210.914541	5946.739379	7.974771	-0.043445	4.171834
210.919020	5954.748823	7.979776	-0.043451	4.174539
211.094180	5962.780946	7.984781	-0.043489	4.177252
211.346097	5970.754733	7.989786	-0.043542	4.179944
211.323196	5978.772423	7.994790	-0.043543	4.182647
211.849604	5986.765356	7.999795	-0.043646	4.185345
211.771074	5994.793458	8.004800	-0.043637	4.188047
211.859556	6002.829701	8.009805	-0.043659	4.190751
212.159329	6010.985178	8.014810	-0.043720	4.193497
212.409221	6018.968323	8.019814	-0.043772	4.196181
212.548715	6026.883910	8.024819	-0.043804	4.198841
212.707351	6034.891464	8.029824	-0.043839	4.201529
213.060530	6042.863691	8.034829	-0.043910	4.204207
213.253336	6050.921609	8.039834	-0.043951	4.206909
213.189067	6058.909723	8.044838	-0.043945	4.209584
213.237174	6066.991836	8.049843	-0.043959	4.212289
213.359519	6074.971406	8.054848	-0.043988	4.214959
213.438494	6082.999447	8.059853	-0.044008	4.217644
213.553778	6090.990418	8.064858	-0.044035	4.220314
213.805640	6098.987107	8.069862	-0.044087	4.222986
214.019241	6107.002275	8.074867	-0.044132	4.225663
214.078620	6115.044959	8.079872	-0.044149	4.228345
214.525301	6123.084262	8.084877	-0.044238	4.231028
214.714290	6131.155105	8.089882	-0.044278	4.233717
214.580514	6139.181358	8.094886	-0.044259	4.236387
214.796949	6147.149998	8.099891	-0.044305	4.239039
214.933146	6155.176751	8.104896	-0.044335	4.241708
215.039961	6163.102265	8.109901	-0.044361	4.244341
215.026710	6171.214885	8.114906	-0.044364	4.247034
215.226718	6179.191140	8.119910	-0.044406	4.249682
215.634317	6187.236419	8.124915	-0.044488	4.252353
215.724184	6195.236283	8.129920	-0.044510	4.255004
215.807524	6203.274372	8.134925	-0.044531	4.257666
216.024355	6211.264836	8.139930	-0.044577	4.260312
216.227930	6219.270164	8.144934	-0.044620	4.262961
216.395326	6227.305154	8.149939	-0.044657	4.265618
216.504407	6235.346776	8.154944	-0.044683	4.268274
216.739595	6243.369324	8.159949	-0.044732	4.270924
216.980155	6251.503806	8.164954	-0.044782	4.273610
217.202441	6259.425138	8.169958	-0.044829	4.276223
217.693935	6267.423161	8.174963	-0.044926	4.278862
217.632428	6275.467970	8.179968	-0.044920	4.281510
217.811705	6283.416721	8.184973	-0.044959	4.284127
218.214280	6291.490158	8.189978	-0.045039	4.286785
218.120864	6299.482328	8.194982	-0.045027	4.289410
218.292175	6307.528910	8.199987	-0.045065	4.292054
218.717848	6315.552395	8.204992	-0.045150	4.294691
218.988452	6323.576203	8.209997	-0.045205	4.297325
219.085451	6331.581624	8.215002	-0.045229	4.299950
219.052644	6339.570312	8.220006	-0.045228	4.302567
219.330962	6347.590793	8.225011	-0.045286	4.305195
219.357508	6355.627966	8.230016	-0.045296	4.307825
219.503383	6363.666320	8.235021	-0.045329	4.310455
219.977823	6371.679087	8.240026	-0.045422	4.313077
219.975141	6379.706001	8.245030	-0.045427	4.315699
220.079334	6387.692308	8.250035	-0.045452	4.318306
220.222225	6395.707507	8.255040	-0.045484	4.320922
220.666082	6403.685431	8.260045	-0.045572	4.323526
220.699963	6411.685139	8.265050	-0.045584	4.326132
220.776119	6419.725208	8.270054	-0.045604	4.328751
220.931145	6427.821245	8.275059	-0.045638	4.331386
221.125989	6435.798502	8.280064	-0.045680	4.333982
221.408256	6443.813344	8.285069	-0.045738	4.336589
221.595847	6451.841874	8.290074	-0.045778	4.339198
221.470962	6459.865549	8.295078	-0.045761	4.341802
221.650653	6467.830845	8.300083	-0.045800	4.344387
221.768754	6475.885075	8.305088	-0.045827	4.346999
221.870413	6483.861656	8.310093	-0.045851	4.349584
222.154772	6491.937689	8.315098	-0.045910	4.352202
222.302562	6500.012767	8.320102	-0.045943	4.354816
222.490621	6508.005065	8.325107	-0.045983	4.357402
222.614541	6515.938730	8.330112	-0.046012	4.359968
222.765610	6523.952963	8.335117	-0.046046	4.362558
222.870505	6531.955508	8.340122	-0.046071	4.365142
222.857043	6539.978660	8.345126	-0.046074	4.367731
223.205025	6547.983268	8.350131	-0.046144	4.370314
223.207662	6556.069968	8.355136	-0.046150	4.372921
223.533493	6564.041098	8.360141	-0.046216	4.375490
223.867233	6572.065415	8.365146	-0.046284	4.378075
223.619604	6580.030424	8.370150	-0.046243	4.380636
223.712078	6588.093939	8.375155	-0.046266	4.383229
223.986766	6596.095864	8.380160	-0.046322	4.385802
224.018352	6604.107851	8.385165	-0.046334	4.388375
224.234967	6612.130102	8.390170	-0.046379	4.390951
224.220991	6620.195197	8.395174	-0.046382	4.393538
224.461038	6628.244172	8.400179	-0.046432	4.396120
224.756122	6636.220053	8.405184	-0.046493	4.398676
224.877708	6644.214309	8.410189	-0.046521	4.401237
224.844209	6652.206061	8.415194	-0.046520	4.403794
224.917588	6660.253450	8.420198	-0.046539	4.406368
225.234946	6668.280180	8.425203	-0.046604	4.408935
225.431393	6676.300926	8.430208	-0.046646	4.411498
225.273269	6684.352507	8.435213	-0.046622	4.414068
225.538722	6692.410997	8.440218	-0.046677	4.416641
225.538460	6700.345159	8.445222	-0.046682	4.419171
225.686284	6708.403155	8.450227	-0.046715	4.421740
225.637372	6716.337443	8.455232	-0.046712	4.424267
225.750533	6724.388660	8.460237	-0.046738	4.426830
226.097508	6732.426493	8.465242	-0.046808	4.429389
226.166944	6740.455400	8.470246	-0.046827	4.431942
226.360657	6748.523586	8.475251	-0.046868	4.434507
226.671332	6756.521156	8.480256	-0.046932	4.437048
226.728421	6764.447217	8.485261	-0.046948	4.439564
226.833688	6772.508087	8.490266	-0.046973	4.442122
227.160100	6780.455465	8.495270	-0.047039	4.444643
227.064665	6788.515519	8.500275	-0.047027	4.447196
227.363697	6796.501124	8.505280	-0.047088	4.449726
227.506566	6804.590084	8.510285	-0.047120	4.452287
227.933375	6812.640723	8.515290	-0.047205	4.454835
227.795427	6820.624074	8.520294	-0.047185	4.457358
227.967420	6828.618030	8.525299	-0.047222	4.459885
228.127894	6836.624644	8.530304	-0.047257	4.462413
228.209666	6844.579401	8.535309	-0.047278	4.464924
228.341913	6852.701462	8.540314	-0.047308	4.467486
228.559255	6860.695520	8.545318	-0.047354	4.470007
228.699080	6868.748577	8.550323	-0.047386	4.472545
228.808121	6876.749082	8.555328	-0.047412	4.475064
228.903955	6884.728487	8.560333	-0.047435	4.477575
229.321350	6892.766612	8.565338	-0.047518	4.480105
229.548230	6900.752811	8.570343	-0.047566	4.482616
229.491607	6908.749452	8.575347	-0.047561	4.485128
229.656557	6916.787141	8.580352	-0.047597	4.487652
229.661131	6924.769296	8.585357	-0.047603	4.490157
229.965028	6932.854615	8.590362	-0.047665	4.492693
230.075131	6940.828886	8.595367	-0.047691	4.495193
230.165121	6948.860668	8.600371	-0.047713	4.497709
230.299249	6956.879637	8.605376	-0.047744	4.500221
230.464541	6964.886903	8.610381	-0.047780	4.502727
230.923506	6972.882193	8.615386	-0.047871	4.505228
230.813821	6980.911883	8.620391	-0.047856	4.507738
230.892271	6988.932469	8.625395	-0.047876	4.510243
231.065411	6997.032812	8.630400	-0.047914	4.512773
231.206088	7005.036949	8.635405	-0.047946	4.515271
231.455895	7013.014708	8.640410	-0.047998	4.517759
231.666040	7020.954183	8.645415	-0.048042	4.520234
231.844545	7029.033665	8.650419	-0.048081	4.522752
231.618088	7036.990190	8.655424	-0.048044	4.525228
231.736194	7045.005833	8.660429	-0.048072	4.527723
232.036873	7053.029753	8.665434	-0.048133	4.530219
232.117076	7061.058648	8.670439	-0.048153	4.532715
232.292284	7069.062258	8.675443	-0.048192	4.535201
232.486655	7077.092350	8.680448	-0.048233	4.537695
232.558079	7085.099489	8.685453	-0.048252	4.540180
232.879901	7093.115665	8.690458	-0.048317	4.542666
233.109551	7101.118741	8.695463	-0.048366	4.545147
232.947385	7109.142481	8.700467	-0.048341	4.547633
233.066428	7117.182228	8.705472	-0.048369	4.550122
233.327315	7125.190415	8.710477	-0.048423	4.552601
233.728177	7133.258961	8.715482	-0.048503	4.555097
233.533487	7141.233767	8.720487	-0.048472	4.557562
233.910056	7149.229551	8.725491	-0.048548	4.560032
234.223269	7157.265489	8.730496	-0.048611	4.562514
234.261871	7165.203798	8.735501	-0.048624	4.564964
234.529254	7173.309559	8.740506	-0.048679	4.567464
234.627840	7181.311067	8.745511	-0.048703	4.569931
234.807911	7189.384582	8.750515	-0.048742	4.572419
235.004548	7197.366176	8.755520	-0.048784	4.574877
235.071084	7205.385004	8.760525	-0.048802	4.577345
235.312256	7213.367099	8.765530	-0.048852	4.579800
235.381758	7221.422082	8.770535	-0.048871	4.582276
235.760242	7229.387216	8.775539	-0.048947	4.584724
235.925545	7237.503664	8.780544	-0.048983	4.587217
235.891348	7245.425576	8.785549	-0.048982	4.589648
235.762802	7253.544255	8.790554	-0.048964	4.592139
236.011565	7261.565857	8.795559	-0.049016	4.594598
236.364421	7269.555027	8.800563	-0.049087	4.597046
236.086546	7277.501447	8.805568	-0.049040	4.599480
236.282817	7285.535145	8.810573	-0.049082	4.601939
236.753666	7293.555645	8.815578	-0.049176	4.604393
237.114533	7301.599070	8.820583	-0.049248	4.606853
237.176012	7309.573500	8.825587	-0.049265	4.609290
237.301813	7317.613510	8.830592	-0.049294	4.611745
237.459307	7325.633311	8.835597	-0.049329	4.614194
237.507196	7333.672777	8.840602	-0.049343	4.616647
237.545392	7341.592634	8.845607	-0.049356	4.619062
237.753239	7349.657117	8.850611	-0.049400	4.621520
238.127032	7357.660495	8.855616	-0.049475	4.623958
238.009115	7365.661642	8.860621	-0.049459	4.626394
238.249523	7373.689947	8.865626	-0.049509	4.628837
238.372195	7381.770698	8.870631	-0.049537	4.631294
238.723398	7389.783204	8.875635	-0.049608	4.633730
238.873254	7397.806921	8.880640	-0.049641	4.636167
238.853386	7405.714282	8.885645	-0.049643	4.638569
238.982297	7413.786567	8.890650	-0.049673	4.641018
239.351369	7421.776218	8.895655	-0.049747	4.643442
239.666659	7429.794782	8.900659	-0.049811	4.645873
239.937294	7437.794884	8.905664	-0.049867	4.648296
239.741645	7445.834023	8.910669	-0.049836	4.650731
240.005517	7453.902448	8.915674	-0.049891	4.653173
240.076173	7461.904400	8.920679	-0.049909	4.655594
240.144970	7469.883694	8.925683	-0.049927	4.658007
240.360769	7477.906963	8.930688	-0.049973	4.660431
240.553632	7485.926143	8.935693	-0.050014	4.662853
240.594330	7493.946891	8.940698	-0.050027	4.665275
240.525800	7501.924796	8.945703	-0.050020	4.667682
240.819736	7509.951897	8.950707	-0.050080	4.670103
241.099733	7518.083714	8.955712	-0.050138	4.672554
241.324687	7526.066242	8.960717	-0.050185	4.674958
241.399084	7534.069849	8.965722	-0.050205	4.677368
241.459860	7542.020481	8.970727	-0.050221	4.679761
241.723478	7550.041714	8.975731	-0.050276	4.682173
241.700047	7558.001187	8.980736	-0.050277	4.684566
241.983505	7566.065235	8.985741	-0.050335	4.686989
242.267520	7574.097184	8.990746	-0.050394	4.689400
242.208830	7582.085492	8.995751	-0.050388	4.691798
242.493091	7590.107124	9.000755	-0.050447	4.694205
242.662094	7598.177011	9.005760	-0.050484	4.696624
242.572052	7606.073293	9.010765	-0.050472	4.698991
242.778274	7614.138216	9.015770	-0.050516	4.701406
242.988499	7622.144824	9.020775	-0.050561	4.703803
242.983012	7630.194716	9.025779	-0.050565	4.706212
243.037271	7638.195943	9.030784	-0.050581	4.708605
243.504143	7646.207597	9.035789	-0.050673	4.710999
243.543610	7654.288057	9.040794	-0.050686	4.713413
243.535524	7662.264592	9.045799	-0.050690	4.715795
243.860539	7670.266770	9.050803	-0.050756	4.718183
244.098823	7678.288097	9.055808	-0.050806	4.720576
244.057695	7686.303827	9.060813	-0.050804	4.722966
244.160161	7694.326985	9.065818	-0.050828	4.725357
244.321181	7702.342208	9.070823	-0.050864	4.727744
244.570819	7710.352936	9.075827	-0.050916	4.730128
244.619309	7718.400531	9.080832	-0.050930	4.732522
244.736564	7726.389897	9.085837	-0.050957	4.734898
244.863406	7734.417041	9.090842	-0.050987	4.737284
244.851039	7742.441630	9.095847	-0.050990	4.739668
245.178502	7750.477961	9.100851	-0.051056	4.742054
245.208340	7758.450127	9.105856	-0.051067	4.744420
245.227647	7766.459864	9.110861	-0.051076	4.746796
245.575124	7774.466662	9.115866	-0.051146	4.749169
245.701483	7782.504666	9.120871	-0.051175	4.751551
246.028122	7790.581695	9.125875	-0.051242	4.753943
245.997566	7798.593441	9.130880	-0.051242	4.756315
246.114710	7806.516982	9.135885	-0.051269	4.758659
246.496926	7814.583820	9.140890	-0.051345	4.761044
246.167525	7822.505804	9.145895	-0.051290	4.763387
246.550403	7830.555474	9.150899	-0.051366	4.765764
246.745204	7838.590065	9.155904	-0.051408	4.768136
246.856243	7846.581134	9.160909	-0.051434	4.770494
246.799604	7854.679908	9.165914	-0.051429	4.772884
247.077778	7862.651529	9.170919	-0.051486	4.775233
247.163480	7870.651139	9.175923	-0.051508	4.777591
247.284551	7878.710337	9.180928	-0.051536	4.779964
247.432532	7886.663662	9.185933	-0.051569	4.782306
247.433060	7894.716538	9.190938	-0.051574	4.784676
247.467175	7902.671969	9.195943	-0.051586	4.787015
247.980535	7910.747505	9.200947	-0.051687	4.789388
248.017895	7918.771529	9.205952	-0.051700	4.791745
248.069345	7926.774216	9.210957	-0.051715	4.794096
248.294206	7934.820648	9.215962	-0.051762	4.796457
248.355721	7942.784619	9.220967	-0.051779	4.798793
248.487476	7950.837686	9.225971	-0.051809	4.801154
248.360282	7958.794927	9.230976	-0.051791	4.803487
248.487945	7966.834562	9.235981	-0.051820	4.805842
248.836537	7974.799562	9.240986	-0.051890	4.808173
248.686481	7982.813974	9.245991	-0.051868	4.810520
248.942306	7990.247454	9.250995	-0.051921	4.812693
249.248537	7994.791548	9.256000	-0.051981	4.814021

249.243710	7997.285778	9.261005	-0.051982	4.814750
249.142462	7998.578424	9.266010	-0.051964	4.815129
249.411000	7999.003593	9.271015	-0.052015	4.815252
249.395245	8000.001927	9.276019	-0.052013	4.815543
249.470434	8000.002109	9.281024	-0.052027	4.815543
249.560338	8000.004668	9.286029	-0.052044	4.815543
249.831348	8000.045432	9.291034	-0.052095	4.815554
249.505976	8000.027320	9.296039	-0.052034	4.815550
249.487256	8000.068689	9.301043	-0.052031	4.815562
249.793175	8000.045941	9.306048	-0.052088	4.815554
249.883918	8000.070943	9.311053	-0.052105	4.815561
249.724072	8000.081169	9.316058	-0.052076	4.815565
249.745422	8000.029206	9.321063	-0.052080	4.815550
249.823676	8000.051867	9.326067	-0.052095	4.815556
249.816199	8000.054971	9.331072	-0.052094	4.815557
249.892409	8000.032742	9.336077	-0.052108	4.815550
249.923546	8000.058905	9.341082	-0.052114	4.815557
250.223035	8000.001875	9.346087	-0.052170	4.815539
250.088515	8000.014651	9.351091	-0.052146	4.815544
250.211984	8000.038052	9.356096	-0.052169	4.815550
250.275583	7999.981439	9.361101	-0.052181	4.815533
250.324241	8000.016433	9.366106	-0.052190	4.815543
250.152619	8000.015786	9.371111	-0.052158	4.815544
250.236048	8000.056689	9.376115	-0.052174	4.815555
250.199683	8000.027280	9.381120	-0.052168	4.815547
250.119135	7999.986467	9.386125	-0.052153	4.815535
250.248899	8000.007835	9.391130	-0.052177	4.815541
250.192063	7999.996247	9.396135	-0.052167	4.815538
250.570301	8000.000315	9.401139	-0.052238	4.815537
250.546462	8000.022376	9.406144	-0.052234	4.815544
250.438086	8000.020627	9.411149	-0.052214	4.815544
250.499989	8000.066519	9.416154	-0.052225	4.815557
250.530283	7999.981592	9.421159	-0.052231	4.815532
250.495359	8000.049398	9.426163	-0.052225	4.815552
250.693890	8000.056937	9.431168	-0.052262	4.815553
250.622519	8000.021615	9.436173	-0.052249	4.815543
250.731191	8000.058659	9.441178	-0.052270	4.815553
250.717580	7999.980490	9.446183	-0.052267	4.815531
250.521496	7999.984783	9.451187	-0.052231	4.815533
250.682959	8000.021622	9.456192	-0.052261	4.815543
250.865300	7999.976562	9.461197	-0.052296	4.815529
250.901867	8000.008156	9.466202	-0.052303	4.815538
250.932124	8000.008672	9.471207	-0.052309	4.815538
250.859522	8000.063046	9.476211	-0.052295	4.815554
250.918962	8000.056563	9.481216	-0.052307	4.815552
250.908585	8000.027578	9.486221	-0.052305	4.815543
251.052746	8000.029957	9.491226	-0.052332	4.815543
251.009356	8000.023929	9.496231	-0.052324	4.815542
251.045302	8000.015994	9.501235	-0.052331	4.815539
250.942252	8000.049577	9.506240	-0.052312	4.815550
250.846599	8000.020265	9.511245	-0.052295	4.815542
250.952951	8000.024162	9.516250	-0.052315	4.815542
250.913079	8000.016056	9.521255	-0.052308	4.815540
251.130113	8000.051668	9.526259	-0.052348	4.815549
250.994428	8000.052675	9.531264	-0.052323	4.815550
251.004971	8000.057142	9.536269	-0.052325	4.815552
251.057757	8000.072980	9.541274	-0.052335	4.815556
251.071267	8000.030500	9.546279	-0.052338	4.815543
251.072970	8000.052979	9.551283	-0.052339	4.815550
251.029569	8000.050155	9.556288	-0.052331	4.815549
250.974290	8000.050341	9.561293	-0.052321	4.815550
250.962498	8000.088620	9.566298	-0.052319	4.815561
251.004585	8000.010294	9.571303	-0.052327	4.815538
251.092887	8000.021372	9.576307	-0.052344	4.815541
251.168428	8000.040786	9.581312	-0.052358	4.815546
251.118111	7999.985514	9.586317	-0.052349	4.815530
251.253212	8000.016582	9.591322	-0.052374	4.815538
251.095256	8000.025770	9.596327	-0.052345	4.815542
251.279502	8000.050166	9.601331	-0.052380	4.815548
251.191560	8000.063703	9.606336	-0.052364	4.815552
251.202427	7999.990206	9.611341	-0.052366	4.815531
251.391673	8000.030705	9.616346	-0.052401	4.815542
251.306485	8000.005836	9.621351	-0.052386	4.815535
251.414618	8000.009762	9.626355	-0.052406	4.815536
251.308989	8000.024078	9.631360	-0.052387	4.815540
251.259761	7999.972027	9.636365	-0.052378	4.815525
251.427788	8000.064515	9.641370	-0.052409	4.815552
251.442203	8000.025253	9.646375	-0.052412	4.815540
251.277062	8000.028983	9.651379	-0.052382	4.815542
251.313955	8000.034949	9.656384	-0.052389	4.815543
251.364923	8000.039008	9.661389	-0.052399	4.815544
251.607311	8000.053675	9.666394	-0.052444	4.815547
251.471510	8000.005549	9.671399	-0.052419	4.815534
251.458161	8000.024577	9.676403	-0.052417	4.815540
251.504638	8000.069151	9.681408	-0.052426	4.815552
251.344587	8000.033445	9.686413	-0.052396	4.815543
251.410270	8000.062311	9.691418	-0.052409	4.815551
251.285824	8000.056025	9.696423	-0.052386	4.815550
251.496910	8000.039205	9.701427	-0.052425	4.815544
251.522587	8000.053532	9.706432	-0.052430	4.815548
251.500495	8000.017946	9.711437	-0.052426	4.815537
251.452611	8000.060976	9.716442	-0.052418	4.815550
251.535438	8000.027106	9.721447	-0.052433	4.815540
251.627827	8000.000869	9.726451	-0.052451	4.815532
251.635267	8000.045872	9.731456	-0.052452	4.815545
251.527556	7999.951209	9.736461	-0.052433	4.815518
251.686527	8000.026460	9.741466	-0.052462	4.815539
251.547755	8000.026349	9.746471	-0.052437	4.815540
251.674817	8000.011359	9.751475	-0.052461	4.815535
251.740949	8000.031688	9.756480	-0.052473	4.815540
251.714071	7999.986411	9.761485	-0.052469	4.815527
251.660251	8000.041093	9.766490	-0.052459	4.815543
251.642797	8000.013059	9.771495	-0.052456	4.815535
251.635653	8000.033258	9.776499	-0.052455	4.815541
251.743034	8000.102325	9.781504	-0.052475	4.815561
251.513358	8000.063344	9.786509	-0.052432	4.815551
251.565834	8000.078109	9.791514	-0.052443	4.815555
251.624669	8000.050255	9.796519	-0.052454	4.815546
251.806123	8000.071402	9.801523	-0.052488	4.815552
251.805120	8000.066067	9.806528	-0.052488	4.815550
251.737839	8000.007312	9.811533	-0.052475	4.815533
251.849146	8000.062558	9.816538	-0.052497	4.815549
251.750982	8000.054566	9.821543	-0.052478	4.815547
251.815591	8000.038555	9.826547	-0.052491	4.815542
251.961463	8000.076210	9.831552	-0.052518	4.815552
251.880724	8000.022575	9.836557	-0.052503	4.815537
251.939854	8000.022496	9.841562	-0.052515	4.815537
251.945337	8000.035424	9.846567	-0.052516	4.815540
252.067710	8000.027835	9.851571	-0.052539	4.815537
251.984209	8000.052125	9.856576	-0.052524	4.815545
251.879890	8000.014126	9.861581	-0.052504	4.815534
252.015518	8000.051613	9.866586	-0.052530	4.815545
251.919529	8000.021226	9.871591	-0.052512	4.815536
251.921730	8000.013808	9.876595	-0.052513	4.815534
252.052965	8000.056564	9.881600	-0.052538	4.815546
252.178204	8000.023387	9.886605	-0.052561	4.815536
252.170409	8000.079891	9.891610	-0.052560	4.815552
252.077949	8000.044221	9.896615	-0.052543	4.815542
251.910593	8000.067139	9.901619	-0.052512	4.815550
252.002166	8000.071863	9.906624	-0.052529	4.815551
252.052635	8000.038532	9.911629	-0.052539	4.815541
252.181663	8000.075912	9.916634	-0.052563	4.815551
252.124778	8000.040824	9.921639	-0.052553	4.815541
252.027760	8000.072370	9.926643	-0.052535	4.815551
252.314698	8000.076018	9.931648	-0.052589	4.815550
252.040825	8000.067286	9.936653	-0.052538	4.815549
251.925559	8000.087853	9.941658	-0.052517	4.815556
251.993423	8000.069759	9.946663	-0.052530	4.815550
252.064409	8000.050648	9.951667	-0.052543	4.815544
252.140328	8000.081819	9.956672	-0.052558	4.815553
251.977585	8000.006548	9.961677	-0.052528	4.815532
252.161914	8000.052309	9.966682	-0.052562	4.815544
252.270698	8000.049838	9.971687	-0.052583	4.815543
252.027588	7999.994614	9.976691	-0.052538	4.815528
252.103551	8000.065305	9.981696	-0.052552	4.815548
252.125886	8000.068897	9.986701	-0.052556	4.815549
252.286147	8000.104652	9.991706	-0.052587	4.815559
252.265710	8000.090454	9.996711	-0.052583	4.815555
252.221744	8000.039555	10.001715	-0.052575	4.815540
252.223978	8000.067384	10.006720	-0.052576	4.815548
251.974614	8000.002446	10.011725	-0.052530	4.815530
252.379602	8000.080655	10.016730	-0.052605	4.815551
252.196067	8000.002908	10.021735	-0.052571	4.815529
252.235954	7999.999310	10.026739	-0.052579	4.815528
252.269351	8000.075713	10.031744	-0.052585	4.815550
252.149033	8000.020361	10.036749	-0.052563	4.815535
252.469798	8000.097194	10.041754	-0.052623	4.815556
252.348716	8000.087758	10.046759	-0.052601	4.815553
252.296806	8000.076249	10.051763	-0.052592	4.815550
252.364592	8000.073108	10.056768	-0.052604	4.815549
252.134879	8000.022375	10.061773	-0.052562	4.815535
252.248686	8000.081936	10.066778	-0.052583	4.815552
252.314365	8000.037104	10.071783	-0.052596	4.815539
252.287322	8000.106110	10.076787	-0.052591	4.815559
252.285971	8000.080476	10.081792	-0.052591	4.815552
252.358881	8000.058192	10.086797	-0.052605	4.815545
252.285290	8000.102938	10.091802	-0.052591	4.815558
252.385407	8000.069351	10.096807	-0.052610	4.815548
252.389250	8000.056618	10.101811	-0.052611	4.815544
252.358013	8000.096717	10.106816	-0.052606	4.815556
252.347934	8000.004717	10.111821	-0.052604	4.815529
252.376044	8000.050059	10.116826	-0.052610	4.815542
252.308010	8000.048968	10.121831	-0.052597	4.815542
252.215917	8000.050688	10.126835	-0.052580	4.815543
252.303508	8000.077777	10.131840	-0.052597	4.815551
252.331048	7999.986393	10.136845	-0.052602	4.815524
252.336778	8000.026028	10.141850	-0.052603	4.815535
252.289635	8000.029551	10.146855	-0.052595	4.815537
252.659568	8000.011059	10.151859	-0.052664	4.815529
252.683239	8000.052056	10.156864	-0.052669	4.815541
252.411271	8000.038015	10.161869	-0.052618	4.815538
252.485655	8000.095864	10.166874	-0.052632	4.815555
252.530789	8000.075262	10.171879	-0.052641	4.815549
252.457044	7999.969403	10.176883	-0.052628	4.815518
252.625142	8000.064032	10.181888	-0.052659	4.815545
252.618552	8000.038312	10.186893	-0.052658	4.815537
252.625823	8000.049134	10.191898	-0.052660	4.815541
252.436630	8000.046060	10.196903	-0.052625	4.815541
252.455222	8000.003662	10.201907	-0.052628	4.815528
252.517746	8000.044226	10.206912	-0.052640	4.815540
252.447494	8000.048439	10.211917	-0.052628	4.815541
252.595652	8000.031659	10.216922	-0.052655	4.815536
252.719701	8000.031575	10.221927	-0.052679	4.815535
252.835978	8000.029227	10.226931	-0.052701	4.815534
252.831536	8000.085786	10.231936	-0.052700	4.815550
252.753338	8000.069575	10.236941	-0.052686	4.815546
252.736355	8000.086409	10.241946	-0.052683	4.815551
252.572030	8000.029268	10.246951	-0.052652	4.815535
252.708912	8000.045415	10.251955	-0.052678	4.815539
252.767601	8000.066691	10.256960	-0.052689	4.815545
252.624906	7999.974657	10.261965	-0.052663	4.815519
252.853477	8000.029688	10.266970	-0.052706	4.815534
252.991239	8000.034101	10.271975	-0.052732	4.815534
252.851097	8000.043578	10.276979	-0.052706	4.815538
252.753724	8000.116775	10.281984	-0.052688	4.815560
252.567887	8000.090257	10.286989	-0.052654	4.815553
252.845720	8000.083076	10.291994	-0.052706	4.815549
252.691084	8000.079500	10.296999	-0.052677	4.815549
252.810440	8000.028069	10.302003	-0.052700	4.815533
252.904270	8000.084100	10.307008	-0.052717	4.815549
252.917009	8000.052287	10.312013	-0.052720	4.815540
252.889446	8000.052926	10.317018	-0.052715	4.815540
252.930399	8000.058959	10.322023	-0.052723	4.815542
252.927978	8000.054668	10.327027	-0.052723	4.815541
253.000176	8000.078302	10.332032	-0.052736	4.815547
252.681118	8000.075239	10.337037	-0.052677	4.815548
252.840312	8000.116318	10.342042	-0.052707	4.815559
252.620442	8000.105265	10.347047	-0.052667	4.815557
252.739686	8000.085876	10.352051	-0.052689	4.815551
252.883421	8000.105340	10.357056	-0.052716	4.815556
252.579485	8000.055527	10.362061	-0.052660	4.815542
252.725361	8000.077162	10.367066	-0.052687	4.815548
252.755240	8000.043493	10.372071	-0.052693	4.815538
252.661811	8000.037714	10.377075	-0.052676	4.815537
252.584530	8000.073855	10.382080	-0.052662	4.815548
252.654180	7999.994908	10.387085	-0.052675	4.815524
252.974313	8000.065324	10.392090	-0.052735	4.815543
252.877998	8000.038135	10.397095	-0.052717	4.815536
252.714923	8000.095302	10.402099	-0.052687	4.815553
252.764184	8000.077972	10.407104	-0.052696	4.815548
252.780546	8000.029129	10.412109	-0.052700	4.815534
252.797234	8000.059331	10.417114	-0.052703	4.815542
252.583475	8000.076149	10.422119	-0.052663	4.815548
252.753474	8000.031956	10.427123	-0.052695	4.815535
252.787545	8000.080600	10.432128	-0.052702	4.815549
252.782754	8000.071999	10.437133	-0.052701	4.815546
252.786186	8000.109461	10.442138	-0.052702	4.815557
252.811605	8000.085332	10.447143	-0.052707	4.815550
252.743650	8000.106672	10.452147	-0.052695	4.815557
253.005521	8000.116321	10.457152	-0.052744	4.815558
252.778825	8000.079521	10.462157	-0.052702	4.815548
252.624061	8000.067397	10.467162	-0.052673	4.815546
252.835732	8000.085836	10.472167	-0.052713	4.815550
252.884200	8000.085583	10.477171	-0.052722	4.815550
252.875488	8000.127119	10.482176	-0.052721	4.815562
252.681373	8000.078035	10.487181	-0.052685	4.815548
252.951844	8000.070734	10.492186	-0.052735	4.815545
252.970125	8000.064646	10.497191	-0.052739	4.815543
252.804636	8000.063028	10.502195	-0.052708	4.815543
252.974003	8000.079707	10.507200	-0.052740	4.815547
252.863396	8000.019172	10.512205	-0.052720	4.815530
252.813835	8000.092083	10.517210	-0.052711	4.815552
252.722580	8000.041479	10.522215	-0.052694	4.815537
252.925497	8000.060843	10.527219	-0.052732	4.815542
253.134421	8000.108077	10.532224	-0.052771	4.815555
253.033200	8000.067990	10.537229	-0.052753	4.815544
253.122116	8000.083353	10.542234	-0.052770	4.815548
252.924996	8000.076944	10.547239	-0.052733	4.815547
253.148316	8000.030419	10.552243	-0.052775	4.815532
253.092787	8000.094688	10.557248	-0.052765	4.815551
253.055362	8000.001170	10.562253	-0.052758	4.815524
252.965436	8000.064876	10.567258	-0.052742	4.815543
252.923649	8000.035375	10.572263	-0.052734	4.815535
253.133452	8000.048443	10.577267	-0.052773	4.815537
253.163432	8000.098090	10.582272	-0.052779	4.815552
253.005390	8000.049595	10.587277	-0.052750	4.815538
253.078083	8000.051875	10.592282	-0.052764	4.815539
253.229849	8000.074675	10.597287	-0.052792	4.815545
252.925318	8000.022716	10.602291	-0.052736	4.815531
253.057646	8000.105012	10.607296	-0.052761	4.815554
252.949797	8000.079770	10.612301	-0.052741	4.815547
253.167362	8000.105784	10.617306	-0.052782	4.815554
252.999358	8000.066740	10.622311	-0.052751	4.815543
253.157755	8000.081103	10.627315	-0.052780	4.815547
253.163765	8000.092973	10.632320	-0.052782	4.815550
253.180872	8000.025983	10.637325	-0.052785	4.815531
253.173084	8000.072875	10.642330	-0.052784	4.815544
253.256944	8000.065724	10.647335	-0.052800	4.815542
253.039113	8000.078203	10.652339	-0.052760	4.815547
253.092615	8000.084441	10.657344	-0.052770	4.815548
253.101709	8000.068590	10.662349	-0.052772	4.815543
253.078820	8000.043670	10.667354	-0.052768	4.815536
253.034656	8000.064332	10.672359	-0.052760	4.815542
252.959774	8000.028948	10.677363	-0.052746	4.815532
253.155263	8000.097325	10.682368	-0.052783	4.815552
252.914765	8000.051754	10.687373	-0.052738	4.815539
253.286797	8000.121953	10.692378	-0.052808	4.815558
253.384081	8000.089387	10.697383	-0.052826	4.815548
253.180977	8000.078607	10.702387	-0.052789	4.815546
252.965669	8000.081514	10.707392	-0.052749	4.815548
253.068020	8000.030873	10.712397	-0.052768	4.815532
253.220250	8000.070771	10.717402	-0.052797	4.815543
253.099063	8000.083763	10.722407	-0.052774	4.815548
253.128568	8000.074654	10.727411	-0.052780	4.815545
253.216672	8000.097481	10.732416	-0.052797	4.815551
253.149395	8000.082516	10.737421	-0.052784	4.815547
253.068570	8000.083351	10.742426	-0.052770	4.815548
253.306449	8000.054155	10.747431	-0.052814	4.815538
253.050689	8000.064944	10.752435	-0.052767	4.815542
253.193046	8000.103612	10.757440	-0.052794	4.815553
253.191879	8000.077980	10.762445	-0.052794	4.815546
253.376140	8000.142970	10.767450	-0.052828	4.815564
253.354935	8000.086033	10.772455	-0.052824	4.815547
253.218454	8000.075276	10.777459	-0.052799	4.815545
253.407872	8000.089080	10.782464	-0.052835	4.815548
253.164361	8000.035982	10.787469	-0.052790	4.815533
253.091863	8000.060452	10.792474	-0.052776	4.815541
253.079030	8000.029288	10.797479	-0.052774	4.815532
253.336205	8000.078381	10.802483	-0.052822	4.815545
253.322186	8000.086719	10.807488	-0.052820	4.815547
253.182059	8000.024631	10.812493	-0.052794	4.815530
253.357709	8000.087344	10.817498	-0.052827	4.815547
253.290390	8000.106558	10.822503	-0.052815	4.815553
253.358678	8000.094880	10.827507	-0.052828	4.815550
253.243498	8000.098357	10.832512	-0.052807	4.815551
253.113034	8000.022543	10.837517	-0.052783	4.815530
253.114800	8000.064251	10.842522	-0.052783	4.815542
253.121353	8000.070789	10.847527	-0.052785	4.815544
252.970086	8000.085425	10.852531	-0.052757	4.815549
253.311086	8000.136958	10.857536	-0.052821	4.815562
253.156716	8000.102409	10.862541	-0.052792	4.815553
253.344090	8000.131133	10.867546	-0.052827	4.815560
253.359996	8000.115393	10.872551	-0.052830	4.815556
253.248442	8000.108248	10.877555	-0.052810	4.815554
253.463724	8000.120340	10.882560	-0.052850	4.815557
253.218241	8000.106730	10.887565	-0.052805	4.815554
253.315188	8000.140383	10.892570	-0.052823	4.815563
253.502009	8000.125305	10.897575	-0.052858	4.815558
253.528086	8000.137503	10.902579	-0.052863	4.815561
253.407521	8000.122733	10.907584	-0.052841	4.815557
253.141825	8000.090634	10.912589	-0.052792	4.815549
253.359101	8000.086736	10.917594	-0.052832	4.815547
253.274287	8000.104596	10.922599	-0.052817	4.815553
253.415933	8000.106936	10.927603	-0.052843	4.815553
253.510369	8000.109572	10.932608	-0.052861	4.815553
253.440652	8000.065727	10.937613	-0.052849	4.815541
253.440042	8000.045445	10.942618	-0.052849	4.815535
253.603057	8000.087656	10.947623	-0.052879	4.815546
253.480344	8000.065375	10.952627	-0.052857	4.815540
253.324937	8000.102374	10.957632	-0.052828	4.815552
253.213948	8000.076012	10.962637	-0.052808	4.815545
253.420005	8000.096497	10.967642	-0.052846	4.815550
253.451037	8000.077800	10.972647	-0.052852	4.815544
253.362500	8000.096667	10.977651	-0.052836	4.815550
253.513992	8000.115191	10.982656	-0.052864	4.815555
253.615946	8000.043181	10.987661	-0.052884	4.815533
253.486078	8000.096620	10.992666	-0.052860	4.815549
253.559837	8000.116007	10.997671	-0.052874	4.815555
253.368734	8000.096879	11.002675	-0.052838	4.815550
253.503918	8000.104454	11.007680	-0.052864	4.815552
253.443871	8000.052222	11.012685	-0.052853	4.815537
253.547962	8000.073175	11.017690	-0.052873	4.815542
253.487395	8000.064728	11.022695	-0.052862	4.815540
253.375463	8000.053305	11.027699	-0.052841	4.815537
253.414059	8000.111638	11.032704	-0.052848	4.815554
253.389875	8000.067470	11.037709	-0.052844	4.815541
253.586591	8000.092075	11.042714	-0.052881	4.815547
253.437853	8000.087526	11.047719	-0.052854	4.815547
253.518644	8000.051485	11.052723	-0.052869	4.815536
253.579368	8000.119794	11.057728	-0.052880	4.815556
253.478035	8000.074363	11.062733	-0.052862	4.815543
253.668838	8000.126643	11.067738	-0.052898	4.815557
253.612586	8000.105450	11.072743	-0.052887	4.815551
253.442321	8000.038596	11.077747	-0.052856	4.815532
253.555451	8000.059696	11.082752	-0.052877	4.815538
253.609487	8000.010400	11.087757	-0.052887	4.815523
253.672749	8000.072341	11.092762	-0.052900	4.815541
253.321738	8000.126433	11.097767	-0.052834	4.815559
253.451427	8000.124305	11.102771	-0.052859	4.815557
253.552176	8000.097137	11.107776	-0.052878	4.815549
253.384254	8000.064502	11.112781	-0.052847	4.815540
253.539853	8000.100183	11.117786	-0.052876	4.815550
253.624532	8000.090910	11.122791	-0.052892	4.815547
253.486785	8000.059837	11.127795	-0.052867	4.815538
253.522477	8000.087147	11.132800	-0.052874	4.815546
253.556772	8000.079185	11.137805	-0.052880	4.815544
253.602882	8000.086370	11.142810	-0.052889	4.815546
253.522956	8000.092561	11.147815	-0.052874	4.815548
253.593564	8000.076648	11.152819	-0.052888	4.815543
253.736157	8000.122799	11.157824	-0.052915	4.815556
253.566412	8000.057021	11.162829	-0.052883	4.815537
253.523210	8000.087312	11.167834	-0.052875	4.815546
253.550107	8000.074956	11.172839	-0.052881	4.815542
253.450282	8000.070139	11.177843	-0.052862	4.815542
253.632455	8000.118006	11.182848	-0.052897	4.815555
253.634955	8000.055048	11.187853	-0.052897	4.815536
253.642945	8000.085109	11.192858	-0.052899	4.815545
253.575503	8000.094708	11.197863	-0.052887	4.815548
253.708953	8000.095847	11.202867	-0.052912	4.815548
253.780965	8000.128024	11.207872	-0.052925	4.815557
253.534108	8000.110118	11.212877	-0.052880	4.815553
253.709661	8000.058539	11.217882	-0.052913	4.815537
253.789187	8000.084430	11.222887	-0.052928	4.815544
253.548404	8000.075169	11.227891	-0.052883	4.815542
253.502197	8000.110751	11.232896	-0.052875	4.815553
253.626224	8000.117076	11.237901	-0.052898	4.815554
253.723485	8000.135781	11.242906	-0.052916	4.815559
253.626127	8000.114982	11.247911	-0.052899	4.815554
253.554276	8000.104214	11.252915	-0.052885	4.815551
253.741045	8000.133998	11.257920	-0.052920	4.815559
253.689152	8000.094717	11.262925	-0.052911	4.815547
253.579657	8000.105764	11.267930	-0.052891	4.815551
253.674434	8000.100928	11.272935	-0.052909	4.815549
253.596172	8000.080442	11.277939	-0.052894	4.815544
253.641860	8000.141028	11.282944	-0.052903	4.815561
253.618099	8000.095799	11.287949	-0.052899	4.815548
253.613047	8000.094670	11.292954	-0.052898	4.815548
253.687674	8000.120481	11.297959	-0.052913	4.815555
253.755315	8000.076748	11.302963	-0.052925	4.815542
253.874016	8000.144939	11.307968	-0.052948	4.815561
253.603089	8000.118094	11.312973	-0.052898	4.815555
253.725379	8000.119050	11.317978	-0.052921	4.815554
253.870210	8000.117171	11.322983	-0.052948	4.815553
253.734585	8000.093609	11.327987	-0.052923	4.815547
253.672570	8000.154568	11.332992	-0.052911	4.815565
253.635640	8000.121940	11.337997	-0.052905	4.815556
253.673929	8000.133271	11.343002	-0.052912	4.815559
253.643574	8000.123182	11.348007	-0.052907	4.815556
253.485525	8000.069346	11.353011	-0.052878	4.815541
253.680923	8000.140928	11.358016	-0.052914	4.815561
253.727239	8000.104323	11.363021	-0.052923	4.815550
253.639106	8000.097561	11.368026	-0.052907	4.815548
253.951989	8000.105911	11.373031	-0.052965	4.815549
253.742587	8000.098231	11.378035	-0.052927	4.815548
253.662238	8000.112960	11.383040	-0.052912	4.815553
253.875502	8000.087633	11.388045	-0.052952	4.815544
253.865772	8000.105654	11.393050	-0.052950	4.815550
253.746984	8000.114413	11.398055	-0.052929	4.815553
253.639622	8000.054997	11.403059	-0.052909	4.815536
253.925636	8000.143018	11.408064	-0.052962	4.815560
253.773709	8000.121325	11.413069	-0.052934	4.815555
253.706750	8000.090342	11.418074	-0.052922	4.815546
253.613310	8000.110197	11.423079	-0.052905	4.815552
253.706312	8000.103197	11.428083	-0.052922	4.815550
253.742554	8000.115562	11.433088	-0.052929	4.815553
253.708782	8000.093667	11.438093	-0.052923	4.815547
253.694628	8000.103071	11.443098	-0.052921	4.815550
253.732509	8000.103713	11.448103	-0.052928	4.815550
253.778593	8000.066036	11.453107	-0.052937	4.815538
253.847027	8000.124859	11.458112	-0.052950	4.815555
253.774413	8000.062807	11.463117	-0.052937	4.815537
253.932948	8000.075038	11.468122	-0.052967	4.815540
254.096346	8000.098031	11.473127	-0.052997	4.815546
253.735080	8000.057956	11.478131	-0.052930	4.815536
253.955545	8000.108586	11.483136	-0.052972	4.815550
253.999649	8000.097581	11.488141	-0.052980	4.815547
253.954153	8000.132107	11.493146	-0.052972	4.815557
253.664749	8000.114572	11.498151	-0.052918	4.815553
253.578947	8000.137756	11.503155	-0.052902	4.815560
253.806261	8000.140432	11.508160	-0.052945	4.815560
253.814389	8000.093588	11.513165	-0.052947	4.815546
253.744204	8000.123437	11.518170	-0.052934	4.815555
253.801878	8000.112654	11.523175	-0.052945	4.815552
253.800187	8000.131875	11.528179	-0.052945	4.815557
253.816852	8000.093716	11.533184	-0.052948	4.815546
253.682544	8000.082994	11.538189	-0.052923	4.815544
253.846495	8000.104927	11.543194	-0.052954	4.815549
253.846701	8000.113497	11.548199	-0.052955	4.815552
253.607113	8000.099983	11.553203	-0.052910	4.815549
253.686527	8000.142963	11.558208	-0.052925	4.815561
253.641460	8000.099521	11.563213	-0.052917	4.815549
253.713689	8000.114611	11.568218	-0.052931	4.815553
253.953854	8000.105748	11.573223	-0.052976	4.815549
253.842959	8000.052683	11.578227	-0.052955	4.815534
253.725504	8000.122348	11.583232	-0.052934	4.815555
253.738172	8000.095873	11.588237	-0.052936	4.815547
253.987790	8000.110664	11.593242	-0.052983	4.815550
253.773971	8000.099707	11.598247	-0.052943	4.815548
253.663683	8000.075492	11.603251	-0.052923	4.815542
253.939532	8000.103530	11.608256	-0.052975	4.815548
253.913997	8000.108475	11.613261	-0.052970	4.815550
253.771569	8000.112573	11.618266	-0.052944	4.815552
253.820557	8000.135829	11.623271	-0.052953	4.815558
253.955617	8000.073973	11.628275	-0.052979	4.815540
253.895719	8000.076219	11.633280	-0.052968	4.815541
253.740855	8000.040592	11.638285	-0.052939	4.815531
253.988052	8000.118364	11.643290	-0.052986	4.815552
253.785038	8000.119334	11.648295	-0.052948	4.815554
253.726844	8000.091699	11.653299	-0.052937	4.815546
253.907340	8000.139539	11.658304	-0.052971	4.815559
253.848363	8000.095869	11.663309	-0.052961	4.815547
253.853977	8000.048984	11.668314	-0.052962	4.815533
253.816830	8000.100737	11.673319	-0.052955	4.815548
253.792901	8000.073664	11.678323	-0.052951	4.815540
253.862495	8000.107938	11.683328	-0.052964	4.815550
253.920483	8000.074728	11.688333	-0.052975	4.815540
254.011064	8000.100801	11.693338	-0.052992	4.815547
254.160080	8000.123559	11.698343	-0.053020	4.815553
253.825557	8000.129852	11.703347	-0.052958	4.815557
254.063492	8000.159406	11.708352	-0.053003	4.815564
254.234864	8000.097077	11.713357	-0.053035	4.815545
253.961882	8000.073401	11.718362	-0.052984	4.815539
253.998913	8000.084711	11.723367	-0.052992	4.815542
253.857498	8000.038623	11.728371	-0.052965	4.815530
253.922609	8000.058938	11.733376	-0.052978	4.815535
253.863419	8000.091103	11.738381	-0.052967	4.815545
254.019358	8000.089406	11.743386	-0.052996	4.815544
253.972174	8000.119632	11.748391	-0.052988	4.815553
253.884399	8000.137443	11.753395	-0.052972	4.815558
253.981646	8000.130512	11.758400	-0.052990	4.815556
254.120103	8000.108234	11.763405	-0.053016	4.815549
254.178354	8000.164754	11.768410	-0.053027	4.815565
254.059102	8000.133983	11.773415	-0.053005	4.815557
254.161648	8000.087617	11.778419	-0.053025	4.815542
254.218693	8000.106732	11.783424	-0.053036	4.815548
253.967387	8000.102638	11.788429	-0.052989	4.815548
254.163362	8000.091983	11.793434	-0.053026	4.815544
254.262685	8000.142767	11.798439	-0.053044	4.815558
254.051936	8000.115838	11.803443	-0.053005	4.815551
253.890473	8000.161283	11.808448	-0.052976	4.815565
254.053096	8000.136196	11.813453	-0.053006	4.815557
253.988042	8000.129811	11.818458	-0.052994	4.815556
253.956770	8000.142139	11.823463	-0.052989	4.815559
253.795151	8000.120287	11.828467	-0.052959	4.815554
254.094180	8000.134820	11.833472	-0.053015	4.815557
254.101923	8000.108264	11.838477	-0.053017	4.815549
254.040368	8000.127573	11.843482	-0.053005	4.815555
254.000358	8000.121599	11.848487	-0.052998	4.815553
253.831755	8000.081474	11.853491	-0.052967	4.815542
253.995272	8000.130105	11.858496	-0.052998	4.815556
253.947676	8000.098371	11.863501	-0.052989	4.815547
253.936359	8000.135593	11.868506	-0.052987	4.815557
253.975879	8000.124512	11.873511	-0.052995	4.815554
254.002652	8000.110018	11.878515	-0.053000	4.815550
254.154485	8000.128549	11.883520	-0.053029	4.815554
253.989000	8000.080998	11.888525	-0.052998	4.815541
253.935326	8000.094027	11.893530	-0.052988	4.815545
254.288463	8000.136150	11.898535	-0.053054	4.815556
254.092537	8000.088100	11.903539	-0.053018	4.815543
253.917060	8000.140793	11.908544	-0.052986	4.815559
253.951901	8000.081568	11.913549	-0.052992	4.815542
254.061037	8000.090854	11.918554	-0.053013	4.815544
254.098383	8000.124601	11.923559	-0.053020	4.815553
253.986377	8000.112107	11.928563	-0.052999	4.815550
254.009089	8000.134932	11.933568	-0.053004	4.815557
253.875789	8000.106067	11.938573	-0.052979	4.815549
254.006522	8000.134934	11.943578	-0.053004	4.815557
254.071599	8000.127476	11.948583	-0.053016	4.815554
254.175016	8000.086465	11.953587	-0.053036	4.815542
254.085090	8000.112787	11.958592	-0.053019	4.815550
253.922685	8000.068491	11.963597	-0.052989	4.815538
254.203619	8000.103022	11.968602	-0.053042	4.815547
254.283329	8000.113963	11.973607	-0.053057	4.815549
254.042891	8000.081206	11.978611	-0.053012	4.815541
254.171424	8000.124992	11.983616	-0.053037	4.815553
253.930027	8000.074061	11.988621	-0.052992	4.815539
254.034508	8000.088612	11.993626	-0.053012	4.815543
254.092216	8000.128033	11.998631	-0.053023	4.815554
254.033524	8000.107866	12.003635	-0.053012	4.815549
254.229753	8000.129261	12.008640	-0.053049	4.815554
254.273576	8000.093683	12.013645	-0.053057	4.815543
254.169478	8000.119772	12.018650	-0.053038	4.815552
254.173246	8000.128401	12.023655	-0.053039	4.815554
254.102156	8000.080259	12.028659	-0.053026	4.815540
254.295380	8000.121900	12.033664	-0.053062	4.815552
254.422049	8000.114383	12.038669	-0.053086	4.815549
254.064350	8000.110683	12.043674	-0.053020	4.815549
254.127342	8000.137372	12.048679	-0.053032	4.815557
254.329937	8000.158871	12.053683	-0.053070	4.815562
254.352575	8000.173150	12.058688	-0.053074	4.815566
254.151963	8000.131432	12.063693	-0.053037	4.815555
254.261261	8000.184516	12.068698	-0.053058	4.815570
254.129142	8000.154602	12.073703	-0.053033	4.815562
254.300148	8000.129652	12.078707	-0.053065	4.815554
254.308306	8000.134080	12.083712	-0.053067	4.815555
254.227650	8000.109281	12.088717	-0.053052	4.815548
254.183347	8000.147032	12.093722	-0.053044	4.815559
254.122032	8000.150322	12.098727	-0.053033	4.815561
254.088144	8000.109198	12.103731	-0.053027	4.815549
254.082692	8000.140108	12.108736	-0.053026	4.815558
254.143558	8000.122968	12.113741	-0.053038	4.815552
254.321547	8000.146200	12.118746	-0.053071	4.815558
254.294497	8000.142574	12.123751	-0.053067	4.815557
254.078264	8000.095260	12.128755	-0.053027	4.815545
254.283696	8000.099715	12.133760	-0.053065	4.815545
254.150785	8000.109309	12.138765	-0.053041	4.815548
254.148843	8000.125322	12.143770	-0.053040	4.815553
254.143442	8000.133801	12.148775	-0.053040	4.815556
254.189912	8000.113220	12.153779	-0.053049	4.815549
254.223122	8000.123400	12.158784	-0.053055	4.815552
254.205065	8000.110308	12.163789	-0.053052	4.815548
254.124023	8000.128229	12.168794	-0.053037	4.815554
254.250778	8000.141009	12.173799	-0.053061	4.815557
254.056061	8000.069479	12.178803	-0.053025	4.815537
253.996272	8000.122998	12.183808	-0.053014	4.815553
254.017005	8000.082769	12.188813	-0.053018	4.815541
254.025501	8000.103226	12.193818	-0.053020	4.815547
254.197715	8000.144522	12.198823	-0.053052	4.815558
254.083998	8000.134136	12.203827	-0.053031	4.815556
254.398978	8000.105136	12.208832	-0.053090	4.815546
254.428288	8000.099229	12.213837	-0.053096	4.815544
254.363286	8000.137708	12.218842	-0.053084	4.815556
254.388027	8000.134931	12.223847	-0.053089	4.815555
254.221266	8000.100176	12.228851	-0.053058	4.815545
254.284037	8000.130067	12.233856	-0.053070	4.815554
254.246737	8000.105978	12.238861	-0.053063	4.815547
254.288072	8000.107745	12.243866	-0.053071	4.815547
254.373645	8000.112373	12.248871	-0.053087	4.815548
254.184564	8000.092207	12.253875	-0.053053	4.815543
254.395494	8000.157638	12.258880	-0.053092	4.815561
254.295717	8000.116503	12.263885	-0.053074	4.815550
254.267866	8000.102182	12.268890	-0.053069	4.815546
254.437944	8000.095377	12.273895	-0.053101	4.815543
254.310750	8000.065543	12.278899	-0.053077	4.815535
254.465353	8000.131119	12.283904	-0.053106	4.815553
254.452940	8000.099961	12.288909	-0.053104	4.815544
254.344436	8000.142000	12.293914	-0.053084	4.815557
254.553109	8000.141168	12.298919	-0.053123	4.815556
254.476666	8000.110028	12.303923	-0.053109	4.815547
254.472819	8000.123874	12.308928	-0.053109	4.815551
254.238878	8000.098700	12.313933	-0.053066	4.815545
254.430897	8000.087981	12.318938	-0.053102	4.815541
254.440010	8000.111652	12.323943	-0.053104	4.815547
254.373881	8000.097773	12.328947	-0.053092	4.815544
254.410624	8000.138987	12.333952	-0.053099	4.815556
254.431503	8000.101965	12.338957	-0.053103	4.815545
254.392103	8000.138727	12.343962	-0.053096	4.815556
254.348759	8000.119880	12.348967	-0.053088	4.815550
254.222052	8000.085782	12.353971	-0.053064	4.815541
254.627239	8000.129827	12.358976	-0.053140	4.815552
254.295059	8000.110521	12.363981	-0.053079	4.815548
254.400726	8000.122955	12.368986	-0.053099	4.815551
254.425796	8000.093479	12.373991	-0.053103	4.815542
254.301129	8000.060482	12.378995	-0.053080	4.815533
254.473545	8000.081487	12.384000	-0.053113	4.815538
254.388118	8000.117495	12.389005	-0.053097	4.815549
254.408764	8000.071924	12.394010	-0.053101	4.815536
254.505700	8000.101306	12.399015	-0.053120	4.815544
254.271751	8000.093223	12.404019	-0.053076	4.815543
254.380053	8000.108905	12.409024	-0.053097	4.815547
254.426058	8000.093658	12.414029	-0.053105	4.815542
254.538746	8000.083776	12.419034	-0.053127	4.815539
254.638245	8000.114269	12.424039	-0.053145	4.815547
254.520812	8000.125185	12.429043	-0.053124	4.815551
254.523383	8000.101749	12.434048	-0.053125	4.815544
254.503069	8000.074734	12.439053	-0.053121	4.815536
254.374971	8000.101498	12.444058	-0.053097	4.815545
254.329493	8000.123207	12.449063	-0.053089	4.815551
254.381063	8000.082415	12.454067	-0.053099	4.815539
254.607288	8000.126733	12.459072	-0.053141	4.815551
254.561717	8000.115327	12.464077	-0.053133	4.815548
254.519634	8000.125341	12.469082	-0.053126	4.815551
254.517841	8000.136015	12.474087	-0.053126	4.815554
254.544880	8000.105503	12.479091	-0.053131	4.815545
254.468699	8000.104277	12.484096	-0.053117	4.815545
254.441885	8000.130564	12.489101	-0.053112	4.815553
254.268320	8000.145901	12.494106	-0.053080	4.815558
254.297365	8000.148535	12.499111	-0.053086	4.815559
254.358463	8000.124990	12.504115	-0.053097	4.815552
254.537496	8000.149308	12.509120	-0.053131	4.815558
254.317514	8000.140386	12.514125	-0.053090	4.815556
254.157698	8000.119631	12.519130	-0.053061	4.815551
254.529349	8000.149241	12.524135	-0.053130	4.815558
254.560344	8000.126270	12.529139	-0.053136	4.815551
254.377808	8000.159620	12.534144	-0.053102	4.815562
254.434131	8000.070838	12.539149	-0.053113	4.815535
254.733123	8000.088576	12.544154	-0.053169	4.815539
254.820377	8000.122073	12.549159	-0.053186	4.815548
254.517141	8000.096831	12.554163	-0.053129	4.815542
254.504690	8000.121217	12.559168	-0.053127	4.815550
254.463756	8000.094932	12.564173	-0.053120	4.815542
254.338812	8000.081158	12.569178	-0.053097	4.815539
254.302997	8000.126524	12.574183	-0.053091	4.815552
254.114017	8000.077520	12.579187	-0.053056	4.815539
254.376203	8000.117086	12.584192	-0.053105	4.815549
254.317136	8000.099049	12.589197	-0.053094	4.815544
254.432092	8000.114840	12.594202	-0.053116	4.815548
254.550064	8000.122136	12.599207	-0.053138	4.815550
254.523084	8000.105693	12.604211	-0.053133	4.815545
254.710381	8000.149374	12.609216	-0.053168	4.815557
254.463524	8000.109034	12.614221	-0.053122	4.815546
254.358093	8000.126556	12.619226	-0.053103	4.815552
254.503115	8000.144976	12.624231	-0.053130	4.815557
254.545981	8000.128609	12.629235	-0.053139	4.815552
254.572279	8000.152562	12.634240	-0.053144	4.815558
254.558155	8000.108557	12.639245	-0.053141	4.815546
254.536827	8000.139207	12.644250	-0.053138	4.815555
254.557878	8000.157733	12.649255	-0.053142	4.815560
254.256633	8000.102615	12.654259	-0.053086	4.815545
254.526086	8000.124142	12.659264	-0.053136	4.815550
254.504912	8000.125953	12.664269	-0.053133	4.815551
254.401359	8000.123211	12.669274	-0.053114	4.815551
254.360406	8000.139652	12.674279	-0.053106	4.815556
254.483183	8000.106436	12.679283	-0.053129	4.815545
254.598274	8000.143593	12.684288	-0.053151	4.815556
254.410012	8000.083917	12.689293	-0.053116	4.815539
254.495177	8000.018039	12.694298	-0.053132	4.815519
254.648530	8000.118846	12.699303	-0.053161	4.815548
254.547190	8000.127889	12.704307	-0.053142	4.815551
254.734549	8000.130981	12.709312	-0.053178	4.815551
254.597862	8000.104195	12.714317	-0.053152	4.815544
254.483644	8000.102346	12.719322	-0.053131	4.815544
254.370058	8000.144302	12.724327	-0.053110	4.815557
254.416831	8000.097022	12.729331	-0.053119	4.815543
254.410891	8000.079856	12.734336	-0.053119	4.815538
254.247314	8000.048358	12.739341	-0.053088	4.815529
254.494860	8000.071662	12.744346	-0.053135	4.815535
254.699685	8000.062221	12.749351	-0.053173	4.815531
254.418735	8000.046959	12.754355	-0.053121	4.815528
254.464408	8000.126774	12.759360	-0.053130	4.815551
254.605474	8000.137652	12.764365	-0.053156	4.815554
254.474827	8000.106693	12.769370	-0.053132	4.815545
254.577024	8000.092366	12.774375	-0.053151	4.815541
254.624976	8000.067537	12.779379	-0.053161	4.815533
254.737615	8000.093973	12.784384	-0.053182	4.815540
254.563844	8000.078330	12.789389	-0.053150	4.815537
254.512674	8000.079650	12.794394	-0.053140	4.815537
254.779103	8000.096854	12.799399	-0.053190	4.815541
254.611731	8000.079180	12.804403	-0.053159	4.815537
254.643179	8000.091467	12.809408	-0.053166	4.815540
254.649470	8000.083046	12.814413	-0.053167	4.815537
254.510387	8000.096812	12.819418	-0.053141	4.815542
254.631671	8000.130867	12.824423	-0.053164	4.815552
254.662969	8000.126060	12.829427	-0.053170	4.815550
254.529545	8000.124965	12.834432	-0.053146	4.815550
254.390256	8000.107750	12.839437	-0.053120	4.815546
254.476410	8000.088888	12.844442	-0.053136	4.815540
254.509804	8000.121502	12.849447	-0.053143	4.815549
254.367637	8000.088218	12.854451	-0.053116	4.815540
254.668759	8000.141241	12.859456	-0.053173	4.815554
254.709917	8000.133392	12.864461	-0.053181	4.815552
254.507966	8000.130105	12.869466	-0.053143	4.815552
254.445928	8000.130179	12.874471	-0.053132	4.815552
254.405929	8000.061182	12.879475	-0.053125	4.815532
254.594345	8000.121972	12.884480	-0.053160	4.815549
254.328185	8000.095202	12.889485	-0.053111	4.815542
254.550326	8000.048659	12.894490	-0.053152	4.815528
254.527326	8000.123076	12.899495	-0.053148	4.815550
254.458720	8000.090997	12.904499	-0.053136	4.815541
254.528946	8000.131692	12.909504	-0.053149	4.815552
254.530230	8000.094349	12.914509	-0.053150	4.815541
254.405952	8000.114767	12.919514	-0.053127	4.815548
254.555603	8000.135399	12.924519	-0.053155	4.815553
254.523879	8000.082560	12.929523	-0.053149	4.815538
254.653583	8000.083639	12.934528	-0.053174	4.815537
254.590146	8000.086894	12.939533	-0.053162	4.815539
254.461089	8000.058098	12.944538	-0.053138	4.815531
254.843929	8000.094300	12.949543	-0.053210	4.815540
254.581688	8000.033413	12.954547	-0.053161	4.815523
254.531723	8000.117002	12.959552	-0.053152	4.815548
254.638797	8000.139074	12.964557	-0.053172	4.815554
254.719558	8000.119055	12.969562	-0.053188	4.815547
254.572089	8000.133752	12.974567	-0.053161	4.815552
254.454005	8000.076294	12.979571	-0.053139	4.815536
254.544227	8000.115180	12.984576	-0.053156	4.815547
254.456235	8000.082783	12.989581	-0.053140	4.815538
254.524137	8000.039054	12.994586	-0.053153	4.815525
254.569806	8000.097506	12.999591	-0.053161	4.815542
254.508842	8000.090120	13.004595	-0.053150	4.815540
254.425334	8000.131501	13.009600	-0.053135	4.815552
254.568182	8000.090067	13.014605	-0.053162	4.815540
254.540009	8000.100310	13.019610	-0.053157	4.815543
254.763820	8000.063407	13.024615	-0.053199	4.815531
254.618839	8000.033281	13.029619	-0.053172	4.815523
254.545181	8000.052392	13.034624	-0.053158	4.815529
254.594386	8000.080992	13.039629	-0.053168	4.815537
254.475348	8000.064110	13.044634	-0.053146	4.815532
254.617743	8000.107055	13.049639	-0.053173	4.815544
254.355782	8000.078218	13.054643	-0.053124	4.815537
254.654085	8000.105558	13.059648	-0.053180	4.815544
254.633199	8000.077465	13.064653	-0.053176	4.815536
254.622080	8000.065555	13.069658	-0.053175	4.815532
254.459147	8000.112044	13.074663	-0.053144	4.815547
254.499086	8000.078538	13.079667	-0.053152	4.815537
254.458833	8000.119560	13.084672	-0.053145	4.815549
254.483570	8000.095419	13.089677	-0.053150	4.815542
254.478203	8000.004558	13.094682	-0.053149	4.815515
254.825596	8000.056202	13.099687	-0.053214	4.815528
254.770107	8000.048906	13.104691	-0.053204	4.815527
254.608738	8000.067648	13.109696	-0.053174	4.815533
254.603522	8000.106039	13.114701	-0.053173	4.815544
254.656769	8000.080228	13.119706	-0.053183	4.815536
254.615003	8000.104134	13.124711	-0.053176	4.815543
254.467863	8000.077177	13.129715	-0.053149	4.815536
254.611848	8000.069944	13.134720	-0.053176	4.815533
254.508188	8000.090700	13.139725	-0.053157	4.815540
254.423991	8000.037002	13.144730	-0.053141	4.815525
254.787102	8000.096381	13.149735	-0.053209	4.815540
254.742219	8000.090327	13.154739	-0.053201	4.815539
254.507765	8000.106803	13.159744	-0.053158	4.815545
254.508435	8000.087609	13.164749	-0.053158	4.815539
254.432168	8000.095995	13.169754	-0.053144	4.815542
254.708796	8000.133663	13.174759	-0.053196	4.815552
254.497803	8000.101387	13.179763	-0.053157	4.815543
254.793894	8000.101987	13.184768	-0.053212	4.815542
254.800268	8000.099977	13.189773	-0.053214	4.815541
254.695428	8000.090804	13.194778	-0.053194	4.815539
254.468889	8000.121296	13.199783	-0.053153	4.815549
254.614899	8000.044664	13.204787	-0.053180	4.815526
254.493001	8000.073667	13.209792	-0.053157	4.815535
254.556749	8000.116392	13.214797	-0.053170	4.815547
254.725158	8000.084991	13.219802	-0.053201	4.815537
254.663090	8000.138473	13.224807	-0.053190	4.815553
254.400796	8000.070107	13.229811	-0.053141	4.815534
254.804418	8000.126946	13.234816	-0.053217	4.815549
254.548939	8000.109964	13.239821	-0.053169	4.815545
254.608941	8000.070378	13.244826	-0.053181	4.815533
254.691847	8000.088849	13.249831	-0.053196	4.815538
254.724555	8000.077657	13.254835	-0.053203	4.815535
254.591052	8000.106469	13.259840	-0.053178	4.815544
254.597444	8000.076687	13.264845	-0.053180	4.815535
254.607650	8000.057648	13.269850	-0.053182	4.815530
254.642750	8000.089223	13.274855	-0.053189	4.815539
254.631246	8000.037783	13.279859	-0.053187	4.815524
254.660074	8000.057505	13.284864	-0.053192	4.815529
254.620977	8000.090000	13.289869	-0.053185	4.815539
254.488260	8000.088916	13.294874	-0.053161	4.815539
254.562925	8000.111524	13.299879	-0.053175	4.815546
254.609656	8000.061039	13.304883	-0.053184	4.815531
254.783030	8000.085265	13.309888	-0.053216	4.815537
254.713242	8000.069189	13.314893	-0.053204	4.815532
254.811405	7999.994978	13.319898	-0.053222	4.815510
254.675919	8000.096394	13.324903	-0.053197	4.815541
254.693471	8000.059317	13.329907	-0.053201	4.815530
254.791185	8000.083372	13.334912	-0.053219	4.815536
254.943407	8000.080547	13.339917	-0.053248	4.815535
254.711857	8000.045798	13.344922	-0.053205	4.815526
254.772601	8000.116247	13.349927	-0.053217	4.815546
254.799826	8000.092146	13.354931	-0.053222	4.815539
254.899345	8000.117299	13.359936	-0.053241	4.815546
254.704519	8000.099174	13.364941	-0.053205	4.815541
254.860764	8000.039801	13.369946	-0.053234	4.815523
254.879787	8000.113840	13.374951	-0.053238	4.815545
254.621905	8000.094682	13.379955	-0.053190	4.815540
254.821009	8000.103307	13.384960	-0.053227	4.815542
254.986655	8000.082542	13.389965	-0.053258	4.815535
254.799568	8000.091249	13.394970	-0.053224	4.815538
254.786579	8000.089990	13.399975	-0.053222	4.815538
254.696548	8000.101355	13.404979	-0.053205	4.815542
254.864458	8000.107333	13.409984	-0.053237	4.815543
254.832584	8000.127128	13.414989	-0.053231	4.815549
254.940410	8000.128917	13.419994	-0.053251	4.815549
254.782552	8000.155193	13.424999	-0.053222	4.815557
254.811458	8000.092665	13.430003	-0.053228	4.815539
254.739978	8000.065880	13.435008	-0.053215	4.815531
254.844739	8000.097527	13.440013	-0.053234	4.815540
254.657631	8000.120120	13.445018	-0.053200	4.815547
254.763215	8000.133622	13.450023	-0.053220	4.815551
254.821484	8000.050211	13.455027	-0.053231	4.815526
254.692599	8000.069485	13.460032	-0.053207	4.815532
254.721955	8000.095625	13.465037	-0.053213	4.815540
254.793865	8000.089348	13.470042	-0.053226	4.815538
255.082757	8000.133626	13.475047	-0.053280	4.815549
254.681893	8000.097170	13.480051	-0.053206	4.815541
254.760756	8000.095280	13.485056	-0.053221	4.815540
254.949190	8000.105867	13.490061	-0.053256	4.815542
254.700822	8000.100751	13.495066	-0.053210	4.815542
254.703580	8000.136068	13.500071	-0.053211	4.815552
254.732965	8000.116276	13.505075	-0.053217	4.815546
254.680022	8000.115430	13.510080	-0.053207	4.815546
254.821114	8000.088923	13.515085	-0.053234	4.815537
254.755203	8000.087865	13.520090	-0.053222	4.815537
254.723669	8000.160007	13.525095	-0.053216	4.815559
254.775565	8000.130970	13.530099	-0.053226	4.815550
254.817507	8000.169066	13.535104	-0.053234	4.815561
254.909581	8000.157778	13.540109	-0.053252	4.815557
254.714500	8000.092648	13.545114	-0.053215	4.815539
254.872097	8000.156139	13.550119	-0.053245	4.815557
254.759024	8000.134013	13.555123	-0.053224	4.815551
254.843861	8000.169607	13.560128	-0.053240	4.815561
254.813730	8000.147771	13.565133	-0.053235	4.815555
254.661149	8000.096156	13.570138	-0.053207	4.815540
254.721027	8000.129205	13.575143	-0.053218	4.815550
254.691807	8000.116998	13.580147	-0.053213	4.815546
254.762673	8000.147022	13.585152	-0.053226	4.815555
254.765087	8000.146016	13.590157	-0.053227	4.815554
254.848337	8000.133515	13.595162	-0.053243	4.815550
254.963460	8000.153583	13.600167	-0.053265	4.815556
254.995903	8000.106067	13.605171	-0.053271	4.815542
254.904959	8000.116349	13.610176	-0.053254	4.815545
254.753695	8000.114961	13.615181	-0.053226	4.815545
254.820874	8000.030628	13.620186	-0.053239	4.815520
254.872909	8000.126572	13.625191	-0.053249	4.815548
254.716510	8000.095190	13.630195	-0.053220	4.815540
254.734590	8000.146781	13.635200	-0.053224	4.815555
254.855795	8000.135971	13.640205	-0.053246	4.815551
254.633478	8000.098168	13.645210	-0.053205	4.815541
254.849340	8000.109204	13.650215	-0.053246	4.815543
254.833341	8000.069441	13.655219	-0.053243	4.815532
254.894110	8000.109981	13.660224	-0.053255	4.815543
254.859586	8000.115847	13.665229	-0.053248	4.815545
254.780101	8000.115634	13.670234	-0.053234	4.815545
255.102700	8000.125215	13.675239	-0.053294	4.815547
255.053136	8000.072083	13.680243	-0.053285	4.815531
254.630880	8000.084414	13.685248	-0.053207	4.815537
254.783724	8000.121122	13.690253	-0.053236	4.815547
254.926194	8000.112797	13.695258	-0.053262	4.815544
255.188222	8000.137408	13.700263	-0.053311	4.815550
254.837892	8000.079348	13.705267	-0.053246	4.815534
254.936100	8000.141866	13.710272	-0.053265	4.815552
254.896689	8000.136969	13.715277	-0.053258	4.815551
254.846608	8000.074215	13.720282	-0.053249	4.815533
254.976496	8000.127639	13.725287	-0.053273	4.815548
254.839026	8000.084817	13.730291	-0.053248	4.815536
254.857775	8000.109714	13.735296	-0.053252	4.815543
255.039200	8000.116982	13.740301	-0.053286	4.815544
254.838940	8000.146836	13.745306	-0.053249	4.815554
254.829891	8000.142437	13.750311	-0.053247	4.815553
254.905102	8000.121259	13.755315	-0.053261	4.815546
254.981772	8000.117197	13.760320	-0.053276	4.815545
254.954479	8000.160567	13.765325	-0.053271	4.815557
254.902830	8000.134106	13.770330	-0.053262	4.815550
254.986054	8000.136560	13.775335	-0.053277	4.815550
255.024271	8000.130799	13.780339	-0.053285	4.815548
255.031906	8000.097832	13.785344	-0.053286	4.815539
255.012962	8000.106089	13.790349	-0.053283	4.815541
254.877056	8000.080383	13.795354	-0.053258	4.815534
254.903377	8000.142792	13.800359	-0.053263	4.815552
254.817762	8000.127524	13.805363	-0.053248	4.815548
254.842828	8000.136503	13.810368	-0.053252	4.815551
254.905963	8000.122604	13.815373	-0.053264	4.815547
254.991637	8000.068484	13.820378	-0.053281	4.815530
255.093974	8000.134275	13.825383	-0.053300	4.815549
255.013781	8000.089186	13.830387	-0.053285	4.815536
255.268063	8000.126490	13.835392	-0.053333	4.815546
255.150110	8000.128851	13.840397	-0.053311	4.815547
255.188208	8000.142316	13.845402	-0.053319	4.815551
254.940573	8000.182076	13.850407	-0.053273	4.815564
255.018366	8000.149190	13.855411	-0.053287	4.815554
255.055233	8000.162634	13.860416	-0.053295	4.815557
255.151940	8000.130059	13.865421	-0.053313	4.815547
255.104535	8000.111144	13.870426	-0.053304	4.815542
255.123894	8000.133916	13.875431	-0.053308	4.815549
255.102768	8000.121841	13.880435	-0.053304	4.815545
255.133243	8000.127704	13.885440	-0.053310	4.815547
254.929402	8000.140408	13.890445	-0.053273	4.815552
254.967073	8000.081228	13.895450	-0.053280	4.815534
255.098472	8000.114381	13.900455	-0.053305	4.815543
254.993285	8000.114816	13.905459	-0.053285	4.815544
255.114501	8000.130711	13.910464	-0.053308	4.815548
255.176868	8000.133891	13.915469	-0.053320	4.815548
255.213405	8000.106738	13.920474	-0.053327	4.815540
255.187239	8000.165083	13.925479	-0.053322	4.815557
255.167512	8000.134871	13.930483	-0.053319	4.815549
255.073380	8000.128010	13.935488	-0.053302	4.815547
255.195633	8000.139649	13.940493	-0.053325	4.815550
255.214030	8000.115404	13.945498	-0.053328	4.815543
255.431184	8000.154236	13.950503	-0.053369	4.815553
255.196378	8000.129045	13.955507	-0.053326	4.815547
255.235388	8000.106206	13.960512	-0.053333	4.815540
255.416382	8000.124149	13.965517	-0.053367	4.815544
255.250830	8000.148162	13.970522	-0.053336	4.815552
255.029399	8000.171260	13.975527	-0.053295	4.815560
254.941213	8000.127109	13.980531	-0.053279	4.815547
255.219528	8000.124215	13.985536	-0.053331	4.815545
255.025848	8000.145631	13.990541	-0.053296	4.815552
255.139377	8000.112263	13.995546	-0.053317	4.815542
255.360426	8000.123385	14.000551	-0.053358	4.815544
255.249901	8000.091686	14.005555	-0.053338	4.815536
255.357189	8000.135126	14.010560	-0.053358	4.815548
255.476804	8000.159541	14.015565	-0.053381	4.815554
255.364662	8000.125678	14.020570	-0.053360	4.815545
255.183717	8000.161190	14.025575	-0.053327	4.815556
255.210853	8000.110383	14.030579	-0.053332	4.815541
255.134329	8000.132651	14.035584	-0.053318	4.815548
255.083338	8000.112610	14.040589	-0.053309	4.815542
254.960936	8000.091398	14.045594	-0.053286	4.815537
255.371732	8000.141949	14.050599	-0.053363	4.815550
255.176124	8000.160129	14.055603	-0.053327	4.815556
255.213069	8000.166097	14.060608	-0.053334	4.815557
255.332149	8000.156321	14.065613	-0.053356	4.815554
255.041244	8000.073596	14.070618	-0.053302	4.815531
255.156798	8000.150286	14.075623	-0.053324	4.815553
255.066049	8000.112501	14.080627	-0.053307	4.815542
255.110074	8000.094017	14.085632	-0.053316	4.815537
255.192894	8000.122101	14.090637	-0.053332	4.815545
255.128116	8000.111448	14.095642	-0.053320	4.815542
255.048254	8000.166776	14.100647	-0.053305	4.815558
254.987578	8000.129484	14.105651	-0.053294	4.815548
255.177992	8000.120877	14.110656	-0.053330	4.815544
255.239794	8000.135798	14.115661	-0.053342	4.815548
254.990033	8000.116772	14.120666	-0.053295	4.815544
255.167869	8000.161368	14.125671	-0.053329	4.815556
255.098013	8000.142086	14.130675	-0.053316	4.815551
255.248637	8000.146713	14.135680	-0.053344	4.815552
255.069514	8000.140594	14.140685	-0.053311	4.815551
255.022177	8000.147318	14.145690	-0.053303	4.815553
254.914429	8000.175483	14.150695	-0.053283	4.815562
254.897435	8000.143181	14.155699	-0.053280	4.815552
254.942396	8000.149281	14.160704	-0.053288	4.815554
255.250958	8000.165042	14.165709	-0.053346	4.815557
255.182842	8000.142583	14.170714	-0.053334	4.815551
255.214177	8000.157005	14.175719	-0.053340	4.815555
255.240861	8000.130759	14.180723	-0.053345	4.815547
255.303546	8000.132877	14.185728	-0.053357	4.815547
255.232073	8000.163773	14.190733	-0.053344	4.815557
255.030807	8000.122041	14.195738	-0.053307	4.815545
255.280167	8000.150719	14.200743	-0.053353	4.815552
255.002585	8000.123759	14.205747	-0.053302	4.815546
254.979566	8000.136222	14.210752	-0.053298	4.815550
255.118226	8000.131039	14.215757	-0.053324	4.815547
255.053770	8000.058435	14.220762	-0.053312	4.815527
255.081988	8000.132625	14.225767	-0.053318	4.815548
255.095427	8000.102958	14.230771	-0.053320	4.815539
255.132997	8000.124959	14.235776	-0.053328	4.815546
255.178520	8000.135341	14.240781	-0.053336	4.815548
255.177049	8000.069110	14.245786	-0.053336	4.815529
255.182584	8000.141861	14.250791	-0.053338	4.815550
255.104701	8000.148084	14.255795	-0.053323	4.815552
255.084990	7999.177881	14.260800	-0.053319	4.815269

255.193192	7995.995844	14.265805	-0.053338	4.814338
255.373900	7990.556411	14.270810	-0.053368	4.812747
255.103311	7983.920518	14.275815	-0.053314	4.810807
255.027852	7976.617400	14.280819	-0.053295	4.808671
255.128731	7969.007925	14.285824	-0.053309	4.806442
254.938013	7961.191769	14.290829	-0.053269	4.804154
254.746756	7953.319759	14.295834	-0.053228	4.801848
254.942050	7945.329678	14.300839	-0.053260	4.799505
254.987415	7937.458256	14.305843	-0.053263	4.797196
254.940401	7929.408448	14.310848	-0.053249	4.794834
254.819172	7921.409395	14.315853	-0.053222	4.792486
254.736867	7913.344745	14.320858	-0.053202	4.790117
254.906066	7905.422546	14.325863	-0.053228	4.787788
254.841032	7897.378816	14.330867	-0.053211	4.785423
254.717637	7889.399832	14.335872	-0.053183	4.783076
254.691041	7881.444155	14.340877	-0.053173	4.780735
254.693501	7873.398447	14.345882	-0.053169	4.778365
254.818035	7865.445210	14.350887	-0.053187	4.776022
254.601169	7857.360122	14.355891	-0.053142	4.773639
254.284462	7849.364673	14.360896	-0.053078	4.771282
254.454331	7841.378350	14.365901	-0.053104	4.768925
254.489896	7833.410120	14.370906	-0.053106	4.766573
254.616826	7825.333855	14.375911	-0.053125	4.764187
254.416210	7817.456249	14.380915	-0.053082	4.761860
254.439479	7809.378293	14.385920	-0.053082	4.759472
254.358490	7801.446689	14.390925	-0.053062	4.757126
254.201127	7793.374732	14.395930	-0.053027	4.754737
254.278199	7785.291604	14.400935	-0.053037	4.752344
254.289597	7777.297145	14.405939	-0.053034	4.749975
254.050417	7769.307131	14.410944	-0.052984	4.747608
253.981076	7761.318792	14.415949	-0.052966	4.745239
254.156349	7753.352804	14.420954	-0.052994	4.742875
254.127775	7745.356050	14.425959	-0.052984	4.740502
254.098971	7737.372776	14.430963	-0.052974	4.738131
254.044313	7729.298725	14.435968	-0.052958	4.735732
254.169361	7721.333416	14.440973	-0.052977	4.733364
254.083549	7713.290309	14.445978	-0.052956	4.730971
254.083190	7705.301398	14.450983	-0.052951	4.728594
254.031081	7697.314996	14.455987	-0.052936	4.726216
253.913505	7689.290149	14.460992	-0.052909	4.723826
253.987493	7681.362188	14.465997	-0.052918	4.721463
253.793370	7673.298783	14.471002	-0.052877	4.719059
253.620424	7665.360056	14.476007	-0.052840	4.716691
253.565586	7657.299822	14.481011	-0.052825	4.714285
253.585888	7649.298670	14.486016	-0.052823	4.711896
253.788229	7641.286267	14.491021	-0.052856	4.709501
253.458117	7633.303104	14.496026	-0.052790	4.707115
253.450958	7625.303529	14.501031	-0.052783	4.704723
253.685291	7617.327484	14.506035	-0.052822	4.702335
253.581519	7609.288434	14.511040	-0.052798	4.699928
253.423788	7601.336540	14.516045	-0.052763	4.697547
253.447100	7593.283710	14.521050	-0.052763	4.695133
253.305380	7585.330771	14.526055	-0.052731	4.692748
253.282568	7577.267195	14.531059	-0.052722	4.690329
253.136692	7569.259050	14.536064	-0.052690	4.687926
253.150406	7561.291332	14.541069	-0.052688	4.685533
252.958328	7553.279798	14.546074	-0.052647	4.683126
253.012616	7545.321546	14.551079	-0.052652	4.680733
253.029573	7537.265468	14.556083	-0.052650	4.678310
252.908379	7529.256435	14.561088	-0.052623	4.675899
252.887188	7521.261394	14.566093	-0.052614	4.673492
253.160216	7513.120585	14.571098	-0.052660	4.671039
253.169840	7505.183676	14.576103	-0.052656	4.668647
252.863945	7497.227776	14.581107	-0.052595	4.666248
252.932498	7489.183467	14.586112	-0.052602	4.663820
253.133925	7481.275139	14.591117	-0.052635	4.661433
252.952384	7473.202000	14.596122	-0.052596	4.658994
252.787150	7465.282976	14.601127	-0.052560	4.656601
252.798072	7457.214860	14.606131	-0.052557	4.654162
252.871193	7449.220293	14.611136	-0.052566	4.651743
252.616994	7441.194899	14.616141	-0.052514	4.649314
252.517644	7433.247393	14.621146	-0.052490	4.646908
252.660156	7425.225331	14.626151	-0.052512	4.644477
252.402231	7417.299169	14.631155	-0.052459	4.642074
252.389412	7409.209999	14.636160	-0.052452	4.639620
252.632019	7401.302502	14.641165	-0.052492	4.637221
252.579786	7393.216567	14.646170	-0.052477	4.634765
252.398037	7385.135777	14.651175	-0.052438	4.632311
252.338030	7377.160140	14.656179	-0.052422	4.629886
252.246835	7369.180465	14.661184	-0.052400	4.627460
252.219803	7361.222517	14.666189	-0.052390	4.625038
252.060655	7353.181515	14.671194	-0.052356	4.622590
252.378521	7345.194281	14.676199	-0.052410	4.620157
252.209814	7337.211997	14.681203	-0.052373	4.617725
252.109622	7329.175658	14.686208	-0.052350	4.615274
252.123712	7321.197851	14.691213	-0.052348	4.612840
252.061984	7313.085214	14.696218	-0.052331	4.610364
252.065169	7305.169068	14.701223	-0.052327	4.607946
251.973248	7297.127422	14.706227	-0.052305	4.605489
251.931005	7289.173782	14.711232	-0.052292	4.603057
251.889089	7281.209064	14.716237	-0.052279	4.600621
251.643882	7273.189688	14.721242	-0.052228	4.598166
251.645988	7265.192697	14.726247	-0.052224	4.595717
251.641899	7257.109321	14.731251	-0.052218	4.593241
251.526805	7249.026442	14.736256	-0.052192	4.590763
251.660054	7241.113353	14.741261	-0.052211	4.588336
251.588422	7233.090944	14.746266	-0.052193	4.585874
251.500421	7225.164403	14.751271	-0.052172	4.583440
251.547295	7217.168619	14.756275	-0.052176	4.580983
251.651215	7209.154617	14.761280	-0.052190	4.578520
251.381760	7201.169339	14.766285	-0.052135	4.576064
251.447138	7193.089020	14.771290	-0.052142	4.573578
251.694167	7185.115874	14.776295	-0.052183	4.571123
251.545086	7177.102727	14.781299	-0.052150	4.568654
251.314588	7169.102382	14.786304	-0.052102	4.566188
251.360650	7161.121566	14.791309	-0.052106	4.563727
251.301185	7153.185942	14.796314	-0.052090	4.561279
251.116441	7145.129784	14.801319	-0.052051	4.558791
250.933124	7137.190257	14.806323	-0.052012	4.556339
250.954651	7129.115764	14.811328	-0.052011	4.553843
251.013804	7121.100018	14.816333	-0.052017	4.551365
250.686769	7113.061332	14.821338	-0.051951	4.548877
250.935280	7105.113874	14.826343	-0.051992	4.546417
250.959179	7097.110388	14.831347	-0.051992	4.543939
250.943376	7089.132642	14.836352	-0.051984	4.541466
250.767410	7081.136035	14.841357	-0.051946	4.538986
250.836711	7073.147421	14.846362	-0.051954	4.536508
250.933852	7065.116725	14.851367	-0.051967	4.534016
250.660915	7057.085765	14.856371	-0.051911	4.531521
250.785375	7049.093868	14.861376	-0.051929	4.529038
250.740864	7041.129551	14.866381	-0.051916	4.526561
250.550763	7033.062285	14.871386	-0.051876	4.524051
250.724358	7025.186471	14.876391	-0.051903	4.521600
250.658735	7017.131235	14.881395	-0.051886	4.519091
250.374954	7009.182326	14.886400	-0.051828	4.516614
250.598029	7001.091795	14.891405	-0.051865	4.514092
250.447555	6992.982679	14.896410	-0.051832	4.511561
250.393330	6985.024381	14.901415	-0.051817	4.509077
250.087915	6977.043620	14.906419	-0.051755	4.506584
250.268059	6969.033276	14.911424	-0.051783	4.504081
250.500114	6961.086763	14.916429	-0.051822	4.501598
250.265594	6953.067917	14.921434	-0.051773	4.499088
250.303259	6945.120954	14.926439	-0.051775	4.496601
250.279696	6937.047401	14.931443	-0.051766	4.494073
250.257461	6929.036168	14.936448	-0.051757	4.491562
250.072618	6921.060876	14.941453	-0.051717	4.489061
249.888878	6913.047317	14.946458	-0.051678	4.486547
250.156237	6905.051664	14.951463	-0.051723	4.484038
250.066003	6897.081965	14.956467	-0.051701	4.481535
249.966599	6889.037398	14.961472	-0.051678	4.479006
249.735256	6881.099094	14.966477	-0.051630	4.476510
249.716211	6873.007240	14.971482	-0.051621	4.473964
249.763185	6865.020413	14.976487	-0.051625	4.471450
249.785319	6857.004654	14.981491	-0.051624	4.468926
249.684187	6848.989885	14.986496	-0.051600	4.466400
249.879649	6841.041569	14.991501	-0.051632	4.463894
249.896745	6833.058211	14.996506	-0.051630	4.461376
249.743232	6825.038901	15.001511	-0.051596	4.458844
249.629522	6817.047444	15.006515	-0.051570	4.456320
249.539719	6809.006939	15.011520	-0.051548	4.453778
249.673055	6800.993909	15.016525	-0.051568	4.451245
249.367022	6792.965385	15.021530	-0.051506	4.448704
249.533377	6785.017257	15.026535	-0.051532	4.446188
249.550505	6777.032184	15.031539	-0.051531	4.443659
249.348172	6769.024073	15.036544	-0.051488	4.441120
249.269527	6761.036662	15.041549	-0.051468	4.438587
249.155055	6753.030736	15.046554	-0.051442	4.436046
249.279235	6745.029058	15.051559	-0.051460	4.433507
249.215020	6736.960907	15.056563	-0.051443	4.430944
249.094918	6728.931648	15.061568	-0.051416	4.428391
249.004099	6720.979271	15.066573	-0.051394	4.425862
248.860162	6712.963610	15.071578	-0.051362	4.423310
249.035940	6704.988044	15.076583	-0.051390	4.420772
248.987628	6696.987084	15.081587	-0.051376	4.418223
248.960287	6688.960094	15.086592	-0.051366	4.415664
248.950617	6680.981535	15.091597	-0.051359	4.413119
249.034564	6672.932766	15.096602	-0.051370	4.410551
248.978573	6664.970062	15.101607	-0.051355	4.408008
248.611984	6656.989637	15.106611	-0.051281	4.405456
248.750241	6648.970604	15.111616	-0.051302	4.402894
248.728521	6641.006645	15.116621	-0.051293	4.400346
248.670647	6633.020614	15.121626	-0.051277	4.397790
248.517421	6625.016503	15.126631	-0.051244	4.395226
248.538262	6616.981039	15.131635	-0.051243	4.392651
248.586863	6608.941046	15.136640	-0.051247	4.390073
248.606325	6600.962698	15.141645	-0.051246	4.387514
248.473145	6592.927531	15.146650	-0.051216	4.384934
248.744316	6585.040549	15.151655	-0.051261	4.382402
248.601953	6576.986796	15.156659	-0.051230	4.379813
248.428928	6568.973371	15.161664	-0.051193	4.377235
248.404625	6560.976549	15.166669	-0.051183	4.374662
248.281926	6552.970773	15.171674	-0.051155	4.372084
248.336265	6544.960628	15.176679	-0.051161	4.369504
248.399236	6536.961814	15.181683	-0.051167	4.366926
248.330663	6528.963460	15.186688	-0.051150	4.364346
248.258513	6521.058917	15.191693	-0.051131	4.361795
248.055967	6512.976976	15.196698	-0.051089	4.359184
248.085571	6505.049927	15.201703	-0.051089	4.356623
247.955677	6497.004254	15.206707	-0.051060	4.354021
247.631975	6488.881493	15.211712	-0.050995	4.351392
247.854828	6480.906917	15.216717	-0.051031	4.348812
247.886903	6472.880206	15.221722	-0.051032	4.346212
247.666964	6464.939613	15.226727	-0.050986	4.343638
247.786528	6456.962053	15.231731	-0.051004	4.341052
247.740256	6448.961933	15.236736	-0.050990	4.338456
247.704406	6440.985632	15.241741	-0.050978	4.335866
247.576954	6432.975738	15.246746	-0.050950	4.333263
247.714468	6424.921745	15.251751	-0.050970	4.330646
247.525252	6416.945955	15.256755	-0.050930	4.328051
247.510942	6408.930880	15.261760	-0.050922	4.325443
247.742000	6400.969811	15.266765	-0.050961	4.322852
247.487042	6392.937201	15.271770	-0.050908	4.320233
247.548517	6384.991418	15.276775	-0.050915	4.317643
247.554060	6376.933029	15.281779	-0.050911	4.315014
247.598486	6368.925511	15.286784	-0.050914	4.312401
247.356500	6360.914217	15.291789	-0.050864	4.309782
247.264525	6352.925383	15.296794	-0.050842	4.307171
247.302845	6344.918312	15.301799	-0.050844	4.304553
247.161790	6336.969984	15.306803	-0.050813	4.301951
247.105013	6328.910112	15.311808	-0.050797	4.299312
247.061992	6320.969205	15.316813	-0.050784	4.296710
247.257682	6312.895908	15.321818	-0.050816	4.294065
247.255040	6304.938018	15.326823	-0.050810	4.291454
247.123583	6296.912104	15.331827	-0.050781	4.288819
247.032915	6288.893964	15.336832	-0.050759	4.286185
247.027384	6280.915690	15.341837	-0.050753	4.283563
247.015396	6272.903558	15.346842	-0.050746	4.280929
247.061989	6264.935658	15.351847	-0.050749	4.278307
246.723562	6256.918104	15.356851	-0.050681	4.275665
246.645746	6248.880873	15.361856	-0.050662	4.273016
246.696154	6240.901167	15.366861	-0.050666	4.270386
246.672005	6232.875342	15.371866	-0.050657	4.267739
246.635824	6224.873748	15.376871	-0.050645	4.265098
246.558068	6216.894310	15.381875	-0.050626	4.262462
246.580061	6208.934158	15.386880	-0.050625	4.259832
246.637958	6200.947741	15.391885	-0.050631	4.257191
246.205294	6192.930631	15.396890	-0.050545	4.254535
246.438074	6184.911691	15.401895	-0.050584	4.251882
246.534387	6176.885438	15.406899	-0.050597	4.249224
246.343959	6168.859006	15.411904	-0.050556	4.246562
246.593995	6160.894930	15.416909	-0.050598	4.243922
246.491370	6152.902447	15.421914	-0.050574	4.241268
246.321214	6144.967687	15.426919	-0.050537	4.238632
246.327943	6136.967121	15.431923	-0.050533	4.235973
246.315132	6128.890493	15.436928	-0.050526	4.233287
246.161322	6120.896267	15.441933	-0.050492	4.230626
246.115193	6112.907737	15.446938	-0.050479	4.227965
246.048095	6104.899586	15.451943	-0.050461	4.225297
245.917246	6096.947102	15.456947	-0.050432	4.222644
246.057720	6088.893333	15.461952	-0.050453	4.219959
246.108081	6080.986664	15.466957	-0.050458	4.217320
246.125480	6072.924275	15.471962	-0.050456	4.214627
246.086879	6064.940648	15.476967	-0.050444	4.211959
245.721924	6056.904913	15.481971	-0.050371	4.209268
245.914889	6048.929078	15.486976	-0.050402	4.206601
245.875681	6040.946795	15.491981	-0.050390	4.203927
245.490681	6032.986930	15.496986	-0.050313	4.201256
245.551636	6024.957776	15.501991	-0.050319	4.198564
245.664645	6016.944200	15.506995	-0.050335	4.195877
245.578635	6008.852805	15.512000	-0.050314	4.193160
245.653481	6000.829368	15.517005	-0.050323	4.190465
245.670958	5992.804561	15.522010	-0.050322	4.187768
245.760731	5984.865159	15.527015	-0.050333	4.185098
245.482915	5976.940916	15.532019	-0.050277	4.182428
245.499438	5968.881550	15.537024	-0.050275	4.179714
245.546561	5960.956983	15.542029	-0.050279	4.177043
245.369510	5952.873697	15.547034	-0.050241	4.174315
245.396820	5944.913812	15.552039	-0.050241	4.171629
245.456038	5936.894206	15.557043	-0.050247	4.168922
245.167087	5928.887846	15.562048	-0.050188	4.166213
245.185619	5920.920688	15.567053	-0.050187	4.163520
245.298123	5912.916737	15.572058	-0.050203	4.160813
245.159328	5904.898926	15.577063	-0.050172	4.158097
245.091552	5896.912524	15.582067	-0.050154	4.155390
244.925548	5888.884136	15.587072	-0.050118	4.152667
245.117019	5880.855972	15.592077	-0.050149	4.149946
244.827515	5872.872870	15.597082	-0.050090	4.147232
244.783378	5864.861650	15.602087	-0.050077	4.144510
244.777425	5856.914046	15.607091	-0.050071	4.141809
244.774508	5848.847653	15.612096	-0.050065	4.139065
244.775010	5840.957054	15.617101	-0.050061	4.136380
244.620394	5832.863662	15.622106	-0.050027	4.133622
244.722853	5824.855251	15.627111	-0.050041	4.130893
244.635860	5816.872729	15.632115	-0.050020	4.128170
244.632744	5808.877810	15.637120	-0.050014	4.125442
244.753995	5800.904627	15.642125	-0.050032	4.122721
244.688619	5792.861376	15.647130	-0.050015	4.119971
244.659563	5784.942657	15.652135	-0.050004	4.117263
244.587120	5776.912212	15.657139	-0.049986	4.114515
244.379035	5768.863104	15.662144	-0.049942	4.111756
244.475228	5760.826205	15.667149	-0.049955	4.109004
244.536599	5752.857881	15.672154	-0.049961	4.106273
244.350662	5744.880634	15.677159	-0.049922	4.103534
244.297827	5736.891870	15.682163	-0.049907	4.100790
244.163399	5728.868930	15.687168	-0.049877	4.098032
244.284436	5720.926886	15.692173	-0.049895	4.095304
244.257602	5712.882449	15.697178	-0.049885	4.092536
244.293318	5704.893606	15.702183	-0.049886	4.089786
244.366555	5696.880565	15.707187	-0.049895	4.087027
244.327643	5688.873726	15.712192	-0.049883	4.084267
244.159158	5680.955284	15.717197	-0.049847	4.081533
244.004380	5672.923228	15.722202	-0.049813	4.078759
244.137965	5664.943869	15.727207	-0.049833	4.076004
243.836952	5656.962998	15.732211	-0.049772	4.073242
243.770590	5648.887032	15.737216	-0.049754	4.070447
244.124213	5640.915868	15.742221	-0.049815	4.067694
243.710256	5632.898458	15.747226	-0.049733	4.064911
243.588339	5624.961161	15.752231	-0.049706	4.062158
243.564314	5616.929873	15.757235	-0.049696	4.059372
243.832994	5608.945927	15.762240	-0.049741	4.056605
243.675170	5600.960837	15.767245	-0.049707	4.053830
243.603181	5592.935487	15.772250	-0.049688	4.051040
243.440291	5584.945551	15.777255	-0.049653	4.048259
243.485651	5576.940721	15.782259	-0.049657	4.045474
243.263380	5568.955442	15.787264	-0.049610	4.042689
243.332654	5560.944524	15.792269	-0.049618	4.039899
243.059862	5552.977041	15.797274	-0.049562	4.037116
243.079501	5544.940882	15.802279	-0.049561	4.034312
242.965848	5536.798108	15.807283	-0.049535	4.031466
243.101525	5528.835166	15.812288	-0.049555	4.028686
243.064222	5520.892358	15.817293	-0.049543	4.025907
242.888709	5512.886198	15.822298	-0.049506	4.023103
242.979143	5504.914992	15.827303	-0.049518	4.020313
243.216011	5496.925897	15.832307	-0.049557	4.017517
242.902516	5488.888388	15.837312	-0.049493	4.014693
242.835241	5480.931066	15.842317	-0.049476	4.011900
242.825635	5472.859435	15.847322	-0.049469	4.009065
242.706409	5464.931659	15.852327	-0.049442	4.006277
242.775186	5456.928199	15.857331	-0.049450	4.003463
242.840142	5448.901251	15.862336	-0.049457	4.000639
242.662148	5440.960139	15.867341	-0.049419	3.997840
242.771048	5432.907937	15.872346	-0.049434	3.995004
242.816022	5424.908596	15.877351	-0.049438	3.992184
242.801860	5416.866336	15.882355	-0.049430	3.989345
242.610341	5408.882210	15.887360	-0.049389	3.986522
242.649602	5400.913402	15.892365	-0.049392	3.983706
242.458743	5392.920376	15.897370	-0.049351	3.980876
242.276891	5384.951215	15.902375	-0.049312	3.978053
242.347685	5376.977659	15.907379	-0.049321	3.975230
242.389857	5368.925687	15.912384	-0.049323	3.972377
242.498109	5360.893948	15.917389	-0.049339	3.969530
242.241012	5352.970639	15.922394	-0.049286	3.966713
242.376790	5344.963975	15.927399	-0.049306	3.963871
242.271283	5336.993915	15.932403	-0.049282	3.961037
241.962246	5328.985037	15.937408	-0.049219	3.958182
242.132933	5320.989514	15.942413	-0.049246	3.955339
242.196529	5312.909390	15.947418	-0.049253	3.952462
241.997404	5304.912745	15.952423	-0.049211	3.949608
241.859828	5296.958319	15.957427	-0.049180	3.946768
241.908516	5288.938447	15.962432	-0.049184	3.943906
241.909763	5280.954681	15.967437	-0.049179	3.941053
241.858900	5272.956591	15.972442	-0.049165	3.938193
241.916416	5264.981620	15.977447	-0.049171	3.935341
241.886143	5256.991525	15.982451	-0.049160	3.932479
241.761342	5248.964975	15.987456	-0.049132	3.929601
241.654347	5241.008745	15.992461	-0.049107	3.926746
241.602330	5232.980775	15.997466	-0.049092	3.923865
241.562873	5224.994594	16.002471	-0.049080	3.920996
241.485983	5217.022269	16.007475	-0.049061	3.918130
241.559644	5209.008194	16.012480	-0.049070	3.915249
241.687229	5200.984215	16.017485	-0.049088	3.912364
241.409319	5192.944551	16.022490	-0.049032	3.909463
241.500871	5184.961132	16.027495	-0.049044	3.906588
241.430063	5176.987665	16.032499	-0.049026	3.903710
241.400288	5168.997224	16.037504	-0.049015	3.900826
241.425568	5160.996008	16.042509	-0.049015	3.897936
241.242701	5152.987479	16.047514	-0.048976	3.895037
241.396743	5144.964650	16.052519	-0.049000	3.892138
241.204676	5136.957429	16.057523	-0.048959	3.889235
241.218804	5128.998731	16.062528	-0.048957	3.886352
241.407696	5120.973793	16.067533	-0.048987	3.883446
241.061135	5113.004926	16.072538	-0.048917	3.880548
241.206741	5105.026923	16.077543	-0.048939	3.877654
241.114866	5097.016942	16.082547	-0.048917	3.874742
241.143532	5088.759366	16.087552	-0.048918	3.871739
241.010902	5080.829066	16.092557	-0.048888	3.868850
240.921238	5072.883562	16.097562	-0.048866	3.865955
240.693068	5064.921656	16.102567	-0.048819	3.863048
240.543779	5056.990609	16.107571	-0.048786	3.860152
240.646556	5048.958527	16.112576	-0.048800	3.857222
240.763247	5040.993249	16.117581	-0.048817	3.854315
240.400613	5032.998187	16.122586	-0.048745	3.851384
240.488916	5024.977470	16.127591	-0.048756	3.848452
240.552811	5016.991471	16.132595	-0.048763	3.845529
240.650988	5008.971279	16.137600	-0.048776	3.842592
240.419826	5001.003771	16.142605	-0.048728	3.839665
240.409696	4993.044436	16.147610	-0.048721	3.836744
240.427432	4985.035216	16.152615	-0.048720	3.833803
240.322090	4977.025543	16.157619	-0.048695	3.830857
240.267344	4969.006476	16.162624	-0.048680	3.827906
240.318103	4961.008784	16.167629	-0.048685	3.824963
240.259335	4953.068410	16.172634	-0.048669	3.822036
240.202949	4945.061218	16.177639	-0.048653	3.819083
240.112078	4937.116372	16.182643	-0.048631	3.816149
239.885239	4929.058788	16.187648	-0.048584	3.813169
240.034765	4921.060888	16.192653	-0.048607	3.810216
239.912222	4913.070650	16.197658	-0.048579	3.807259
239.997676	4905.062707	16.202663	-0.048590	3.804296
240.093690	4897.114269	16.207667	-0.048603	3.801354
240.047275	4889.095313	16.212672	-0.048590	3.798381
240.061934	4881.119430	16.217677	-0.048587	3.795422
239.870477	4873.057762	16.222682	-0.048547	3.792424
239.678952	4865.068069	16.227687	-0.048506	3.789451
239.795718	4857.043680	16.232691	-0.048523	3.786470
239.686469	4849.057545	16.237696	-0.048497	3.783495
239.605229	4841.107901	16.242701	-0.048477	3.780532
239.494641	4833.122763	16.247706	-0.048452	3.777553
239.589361	4825.102290	16.252711	-0.048465	3.774563
239.534974	4817.085475	16.257715	-0.048449	3.771569
239.256713	4809.086171	16.262720	-0.048393	3.768574
239.352153	4801.062202	16.267725	-0.048405	3.765575
239.060701	4793.096626	16.272730	-0.048346	3.762588
239.117300	4785.076973	16.277735	-0.048352	3.759585
239.367588	4777.138360	16.282739	-0.048393	3.756615
239.273428	4769.099930	16.287744	-0.048371	3.753598
239.207442	4761.088709	16.292749	-0.048354	3.750588
239.193864	4753.111422	16.297754	-0.048346	3.747591
239.240606	4745.078676	16.302759	-0.048350	3.744571
239.032005	4737.176999	16.307763	-0.048306	3.741592
239.075781	4729.123360	16.312768	-0.048309	3.738560
239.017514	4721.152208	16.317773	-0.048294	3.735554
239.001356	4713.103779	16.322778	-0.048286	3.732517
238.797494	4705.128355	16.327783	-0.048243	3.729501
238.997930	4697.158562	16.332787	-0.048275	3.726494
238.902826	4689.142991	16.337792	-0.048252	3.723460
238.670456	4681.228523	16.342797	-0.048204	3.720459
238.567171	4673.200230	16.347802	-0.048180	3.717415
238.632082	4665.185855	16.352807	-0.048187	3.714379
238.500190	4657.082140	16.357811	-0.048157	3.711301
238.413924	4649.086628	16.362816	-0.048136	3.708262
238.440390	4641.128168	16.367821	-0.048136	3.705238
238.348389	4633.169141	16.372826	-0.048114	3.702209
238.262116	4625.167935	16.377831	-0.048093	3.699161
238.251089	4617.247892	16.382835	-0.048086	3.696143
238.186095	4609.162730	16.387840	-0.048069	3.693059
238.216259	4601.158227	16.392845	-0.048070	3.690005
238.342837	4593.189925	16.397850	-0.048088	3.686964
238.280468	4585.193313	16.402855	-0.048072	3.683906
238.052236	4577.264153	16.407859	-0.048025	3.680867
237.971334	4569.240547	16.412864	-0.048004	3.677793
238.100616	4561.233260	16.417869	-0.048024	3.674727
238.029667	4553.210222	16.422874	-0.048005	3.671648
237.901613	4545.207545	16.427879	-0.047977	3.668573
237.828115	4537.224209	16.432883	-0.047958	3.665504
237.916143	4529.192038	16.437888	-0.047969	3.662418
237.791404	4521.275096	16.442893	-0.047941	3.659368
237.579050	4513.285696	16.447898	-0.047897	3.656286
237.795943	4505.239864	16.452903	-0.047932	3.653190
237.838097	4497.230504	16.457907	-0.047935	3.650101
237.675378	4489.229029	16.462912	-0.047900	3.647007
237.969721	4481.240945	16.467917	-0.047950	3.643928
237.755299	4473.273592	16.472922	-0.047905	3.640841
237.751485	4465.268708	16.477927	-0.047899	3.637742
237.843405	4457.284956	16.482931	-0.047911	3.634651
237.660954	4449.224834	16.487936	-0.047872	3.631520
237.585846	4441.259946	16.492941	-0.047853	3.628427
237.437295	4433.245166	16.497946	-0.047821	3.625310
237.533088	4425.269984	16.502951	-0.047834	3.622212
237.380218	4417.299021	16.507955	-0.047800	3.619106
237.166788	4409.317609	16.512960	-0.047755	3.615992
237.276628	4401.325923	16.517965	-0.047771	3.612880
237.289679	4393.263150	16.522970	-0.047768	3.609735
236.952344	4385.337807	16.527975	-0.047701	3.606631
236.957695	4377.334328	16.532979	-0.047697	3.603503
237.027953	4369.341938	16.537984	-0.047705	3.600379
236.973245	4361.394112	16.542989	-0.047690	3.597266
236.797592	4353.360738	16.547994	-0.047652	3.594113
236.963666	4345.343296	16.552999	-0.047678	3.590974
236.937808	4337.364152	16.558003	-0.047668	3.587841
236.756127	4329.346089	16.563008	-0.047629	3.584686
236.801157	4321.413149	16.568013	-0.047633	3.581568
236.733088	4313.390670	16.573018	-0.047615	3.578409
236.769887	4305.399343	16.578023	-0.047617	3.575263
236.760128	4297.393911	16.583027	-0.047610	3.572106
236.540359	4289.374600	16.588032	-0.047564	3.568935
236.521071	4281.419669	16.593037	-0.047556	3.565793
236.482863	4273.421056	16.598042	-0.047544	3.562630
236.487463	4265.422458	16.603047	-0.047540	3.559466
236.414872	4257.479255	16.608051	-0.047521	3.556318
236.204167	4249.377821	16.613056	-0.047477	3.553101
236.308648	4241.338197	16.618061	-0.047491	3.549915
236.311102	4233.346384	16.623066	-0.047487	3.546741
236.055481	4225.383427	16.628071	-0.047434	3.543569
236.144689	4217.418283	16.633075	-0.047446	3.540403
235.974914	4209.419387	16.638080	-0.047409	3.537214
236.092480	4201.428794	16.643085	-0.047426	3.534033
235.965644	4193.422388	16.648090	-0.047398	3.530836
236.071707	4185.447043	16.653095	-0.047413	3.527655
236.002420	4177.428156	16.658099	-0.047395	3.524449
235.703948	4169.507433	16.663104	-0.047334	3.521272
235.611134	4161.511227	16.668109	-0.047312	3.518068
235.834285	4153.473976	16.673114	-0.047349	3.514855
235.667773	4145.470825	16.678119	-0.047313	3.511640
235.675303	4137.458559	16.683123	-0.047309	3.508424
235.471021	4129.460688	16.688128	-0.047266	3.505204
235.747171	4121.520731	16.693133	-0.047312	3.502020
235.573775	4113.523552	16.698138	-0.047275	3.498795
235.635209	4105.529490	16.703143	-0.047282	3.495577
235.535121	4097.538349	16.708147	-0.047258	3.492351
235.236813	4089.533041	16.713152	-0.047198	3.489110
235.575514	4081.558727	16.718157	-0.047256	3.485899
235.574648	4073.565062	16.723162	-0.047251	3.482667
235.432963	4065.564482	16.728167	-0.047219	3.479424
235.259633	4057.653265	16.733171	-0.047182	3.476213
235.263777	4049.583019	16.738176	-0.047178	3.472941
235.261269	4041.571651	16.743181	-0.047172	3.469689
235.167534	4033.584277	16.748186	-0.047150	3.466441
234.988021	4025.590563	16.753191	-0.047112	3.463184
234.926595	4017.601143	16.758195	-0.047095	3.459930
234.867727	4009.622131	16.763200	-0.047079	3.456677
234.756068	4001.635775	16.768205	-0.047054	3.453417
234.741072	3993.614830	16.773210	-0.047046	3.450142
235.063900	3985.587215	16.778215	-0.047101	3.446873
235.060678	3977.637718	16.783219	-0.047095	3.443621
234.886730	3969.633358	16.788224	-0.047058	3.440339
234.882056	3961.709773	16.793229	-0.047052	3.437092
234.692195	3953.671068	16.798234	-0.047012	3.433789
234.839022	3945.636242	16.803239	-0.047034	3.430495
234.840222	3937.665799	16.808243	-0.047030	3.427220
234.615153	3929.671487	16.813248	-0.046983	3.423924
234.631822	3921.705256	16.818253	-0.046981	3.420644
234.711126	3913.710450	16.823258	-0.046991	3.417352
234.599286	3905.693734	16.828263	-0.046965	3.414041
234.226487	3897.743507	16.833267	-0.046890	3.410746
234.207318	3889.731754	16.838272	-0.046882	3.407434
234.645042	3881.699566	16.843277	-0.046958	3.404126
234.409296	3873.791471	16.848282	-0.046910	3.400842
234.133409	3865.802646	16.853287	-0.046853	3.397521
234.260438	3857.787985	16.858291	-0.046872	3.394200
234.161204	3849.657385	16.863296	-0.046848	3.390820
234.240792	3841.686499	16.868301	-0.046858	3.387508
234.155401	3833.747798	16.873306	-0.046838	3.384202
234.245065	3825.772126	16.878311	-0.046849	3.380882
234.149433	3817.817718	16.883315	-0.046827	3.377562
233.953558	3809.805690	16.888320	-0.046785	3.374211
234.116126	3801.794333	16.893325	-0.046810	3.370869
234.036776	3793.813742	16.898330	-0.046791	3.367529
233.922701	3785.814269	16.903335	-0.046764	3.364176
234.134659	3777.861134	16.908339	-0.046799	3.360851
233.741061	3769.880055	16.913344	-0.046721	3.357488
233.623165	3761.894553	16.918349	-0.046694	3.354131
233.640436	3753.860891	16.923354	-0.046692	3.350755
233.832000	3745.851385	16.928359	-0.046723	3.347392
233.619043	3737.854554	16.933363	-0.046678	3.344016
233.326564	3729.890579	16.938368	-0.046619	3.340648
233.760523	3721.908455	16.943373	-0.046695	3.337295
233.632432	3713.886468	16.948378	-0.046666	3.333901
233.289755	3705.885590	16.953383	-0.046597	3.330505
233.550693	3697.927816	16.958387	-0.046641	3.327146
233.584625	3689.939738	16.963392	-0.046642	3.323763
233.355105	3681.996966	16.968397	-0.046594	3.320385
233.197601	3673.995037	16.973402	-0.046560	3.316981
233.234962	3665.962869	16.978407	-0.046562	3.313569
233.078096	3657.951051	16.983411	-0.046528	3.310154
232.931865	3649.969344	16.988416	-0.046496	3.306749
233.173050	3641.989240	16.993421	-0.046536	3.303355
233.078872	3634.038382	16.998426	-0.046513	3.299958
232.963675	3626.067696	17.003431	-0.046487	3.296549
232.725685	3618.044825	17.008435	-0.046437	3.293108
232.803415	3609.975857	17.013440	-0.046447	3.289656
232.649756	3602.073027	17.018445	-0.046413	3.286263
232.670904	3594.069571	17.023450	-0.046412	3.282830
232.755341	3586.068032	17.028455	-0.046423	3.279397
232.774986	3578.127155	17.033459	-0.046422	3.275984
232.668444	3570.063904	17.038464	-0.046397	3.272509
232.943771	3562.052017	17.043469	-0.046443	3.269068
232.835426	3554.092103	17.048474	-0.046418	3.265631
232.714702	3546.135975	17.053479	-0.046391	3.262191
232.675757	3538.153378	17.058483	-0.046379	3.258740
232.690084	3530.175093	17.063488	-0.046376	3.255288
232.356735	3522.173841	17.068493	-0.046309	3.251809
232.202880	3514.169813	17.073498	-0.046276	3.248333
232.355076	3506.150483	17.078503	-0.046299	3.244858
232.450100	3498.200257	17.083507	-0.046312	3.241407
232.167322	3490.211712	17.088512	-0.046254	3.237921
231.920819	3482.240722	17.093517	-0.046203	3.234440
232.052645	3474.143000	17.098522	-0.046223	3.230915
231.929052	3466.167975	17.103527	-0.046195	3.227430
232.048063	3458.191085	17.108531	-0.046212	3.223949
231.948307	3450.224701	17.113536	-0.046189	3.220461
232.022505	3442.259220	17.118541	-0.046197	3.216977
232.021472	3434.253174	17.123546	-0.046192	3.213468
232.056026	3426.244700	17.128551	-0.046194	3.209955
231.978328	3418.286126	17.133555	-0.046174	3.206456
231.842963	3410.291361	17.138560	-0.046144	3.202935
231.863184	3402.328264	17.143565	-0.046143	3.199430
231.855883	3394.361633	17.148570	-0.046137	3.195919
231.800834	3386.361635	17.153575	-0.046121	3.192387
231.649743	3378.361319	17.158579	-0.046088	3.188847
231.670041	3370.323938	17.163584	-0.046087	3.185293
231.642427	3362.397379	17.168589	-0.046077	3.181783
231.571788	3354.383030	17.173594	-0.046059	3.178229
231.430307	3346.399271	17.178599	-0.046028	3.174681
231.484620	3338.418981	17.183603	-0.046033	3.171138
231.281729	3330.412784	17.188608	-0.045990	3.167570
231.294388	3322.417279	17.193613	-0.045987	3.164011
231.282295	3314.472374	17.198618	-0.045980	3.160469
231.089298	3306.506405	17.203623	-0.045939	3.156907
231.024761	3298.507681	17.208627	-0.045922	3.153331
231.032371	3290.442646	17.213632	-0.045919	3.149725
231.074315	3282.500577	17.218637	-0.045922	3.146171
230.989731	3274.503278	17.223642	-0.045901	3.142583
230.988915	3266.510414	17.228647	-0.045896	3.138997
231.232330	3258.536706	17.233651	-0.045936	3.135425
230.818639	3250.555532	17.238656	-0.045854	3.131818
230.750658	3242.567655	17.243661	-0.045837	3.128218
230.765374	3234.560755	17.248666	-0.045834	3.124609
230.598452	3226.614978	17.253671	-0.045798	3.121016
230.728396	3218.628243	17.258675	-0.045818	3.117413
230.561997	3210.622911	17.263680	-0.045782	3.113784
230.824949	3202.613823	17.268685	-0.045826	3.110169
230.601635	3194.656978	17.273690	-0.045779	3.106551
230.401134	3186.679051	17.278695	-0.045737	3.102921
230.579904	3178.694508	17.283699	-0.045765	3.099300
230.370175	3170.726004	17.288704	-0.045721	3.095665
230.391231	3162.704014	17.293709	-0.045720	3.092011
230.296371	3154.716183	17.298714	-0.045698	3.088364
230.255122	3146.725589	17.303719	-0.045685	3.084713
230.292882	3138.774017	17.308723	-0.045687	3.081080
230.206552	3130.781676	17.313728	-0.045666	3.077418
230.340111	3122.779955	17.318733	-0.045686	3.073757
230.008341	3114.724224	17.323738	-0.045619	3.070046
230.092512	3106.746016	17.328743	-0.045630	3.066385
229.945466	3098.802958	17.333747	-0.045598	3.062725
230.092812	3090.791896	17.338752	-0.045620	3.059043
229.959085	3082.845633	17.343757	-0.045590	3.055374
230.032967	3074.828163	17.348762	-0.045599	3.051677
229.961870	3066.854880	17.353767	-0.045581	3.047989
229.743859	3058.902395	17.358771	-0.045535	3.044299
229.694619	3050.926730	17.363776	-0.045521	3.040602
230.048435	3042.930496	17.368781	-0.045582	3.036910
229.635125	3034.967616	17.373786	-0.045500	3.033192
229.586316	3026.936569	17.378791	-0.045486	3.029456
229.584980	3018.979545	17.383795	-0.045481	3.025752
229.395095	3011.015118	17.388800	-0.045441	3.022030
229.451459	3003.032861	17.393805	-0.045446	3.018308
229.388720	2995.044180	17.398810	-0.045429	3.014572
229.391345	2987.018564	17.403815	-0.045425	3.010818
229.330697	2979.054236	17.408819	-0.045409	3.007084
229.146402	2971.056968	17.413824	-0.045369	3.003324
229.300019	2963.087987	17.418829	-0.045393	2.999590
229.264434	2955.133583	17.423834	-0.045382	2.995848
228.904608	2947.122058	17.428839	-0.045310	2.992058
228.946989	2939.145069	17.433843	-0.045313	2.988300
228.963839	2931.112055	17.438848	-0.045311	2.984510
228.825973	2923.188234	17.443853	-0.045280	2.980759
228.816066	2915.202789	17.448858	-0.045273	2.976980
228.845607	2907.211421	17.453863	-0.045274	2.973195
228.745431	2899.223049	17.458867	-0.045250	2.969401
228.484539	2891.231298	17.463872	-0.045197	2.965592
228.662624	2883.270376	17.468877	-0.045225	2.961815
228.737602	2875.269022	17.473882	-0.045234	2.958008
228.706404	2867.288719	17.478887	-0.045223	2.954202
228.708591	2859.290934	17.483891	-0.045219	2.950383
228.645778	2851.308575	17.488896	-0.045202	2.946564
228.571736	2843.353459	17.493901	-0.045183	2.942753
228.304522	2835.378886	17.498906	-0.045129	2.938917
228.247856	2827.406920	17.503911	-0.045113	2.935088
228.424581	2819.400482	17.508915	-0.045141	2.931250
228.391003	2811.396267	17.513920	-0.045130	2.927396
228.406273	2803.440654	17.518925	-0.045128	2.923564
228.168143	2795.487649	17.523930	-0.045078	2.919715
228.076126	2787.518248	17.528935	-0.045056	2.915860
228.147753	2779.441479	17.533939	-0.045065	2.911957
228.002358	2771.423227	17.538944	-0.045033	2.908065
228.036858	2763.444829	17.543949	-0.045034	2.904197
228.111007	2755.500927	17.548954	-0.045043	2.900343
228.112183	2747.544827	17.553959	-0.045038	2.896474
228.009287	2739.569893	17.558963	-0.045014	2.892585
227.964581	2731.571765	17.563968	-0.045001	2.888683
227.972795	2723.595832	17.568973	-0.044997	2.884789
227.977355	2715.661061	17.573978	-0.044993	2.880909
227.778466	2707.687047	17.578983	-0.044951	2.876994
227.612818	2699.713912	17.583987	-0.044916	2.873076
227.801072	2691.669518	17.588992	-0.044946	2.869137
227.822513	2683.694769	17.593997	-0.044945	2.865218
227.565982	2675.744424	17.599002	-0.044892	2.861290
227.398003	2667.778709	17.604007	-0.044856	2.857353
227.507877	2659.792717	17.609011	-0.044871	2.853417
227.391497	2651.763102	17.614016	-0.044845	2.849441
227.425944	2643.822216	17.619021	-0.044846	2.845512
227.345831	2635.872542	17.624026	-0.044826	2.841567
227.300127	2627.889820	17.629031	-0.044813	2.837602
227.331543	2619.909507	17.634035	-0.044814	2.833636
227.161178	2611.884377	17.639040	-0.044777	2.829632
227.219467	2603.905928	17.644045	-0.044783	2.825658
227.082253	2595.945401	17.649050	-0.044752	2.821676
227.269481	2587.962144	17.654055	-0.044782	2.817696
227.127429	2580.006655	17.659059	-0.044751	2.813705
226.963083	2571.991040	17.664064	-0.044715	2.809677
226.917902	2564.023624	17.669069	-0.044702	2.805674
226.852214	2556.069344	17.674074	-0.044685	2.801671
226.750649	2548.110785	17.679079	-0.044661	2.797658
226.664529	2540.148300	17.684083	-0.044640	2.793638
226.716326	2532.108436	17.689088	-0.044645	2.789581
226.643349	2524.155797	17.694093	-0.044626	2.785556
226.711343	2516.166268	17.699098	-0.044634	2.781514
226.695042	2508.196285	17.704103	-0.044626	2.777471
226.633505	2500.253634	17.709107	-0.044609	2.773433
226.701573	2492.212983	17.714112	-0.044617	2.769347
226.458463	2484.298359	17.719117	-0.044567	2.765301
226.508594	2476.315208	17.724122	-0.044571	2.761232
226.490021	2468.335378	17.729127	-0.044563	2.757154
226.435974	2460.333731	17.734131	-0.044548	2.753056
226.313751	2452.289351	17.739136	-0.044520	2.748927
226.176621	2444.342165	17.744141	-0.044490	2.744840
226.329302	2436.371419	17.749146	-0.044513	2.740753
226.334278	2428.407537	17.754151	-0.044509	2.736654
226.132856	2420.475822	17.759155	-0.044467	2.732553
225.815309	2412.488346	17.764160	-0.044403	2.728410
225.867166	2404.506032	17.769165	-0.044407	2.724285
225.850345	2396.572272	17.774170	-0.044399	2.720176
225.836521	2388.590601	17.779175	-0.044392	2.716036
225.729025	2380.597472	17.784179	-0.044367	2.711877
225.767625	2372.570384	17.789184	-0.044369	2.707704
226.007047	2364.592631	17.794189	-0.044409	2.703562
225.741933	2356.676814	17.799194	-0.044354	2.699415
225.641725	2348.705119	17.804199	-0.044331	2.695242
225.681656	2340.731914	17.809203	-0.044333	2.691071
225.441812	2332.759593	17.814208	-0.044284	2.686876
225.342909	2324.804204	17.819213	-0.044260	2.682693
225.472151	2316.830685	17.824218	-0.044279	2.678508
225.251328	2308.858114	17.829223	-0.044233	2.674294
225.211797	2300.848417	17.834227	-0.044221	2.670066
225.411859	2292.813419	17.839232	-0.044253	2.665833
225.300374	2284.897405	17.844237	-0.044228	2.661637
225.140056	2276.951050	17.849242	-0.044193	2.657414
225.093899	2268.962917	17.854247	-0.044179	2.653170
225.074210	2260.980241	17.859251	-0.044171	2.648924
224.939545	2253.002511	17.864256	-0.044141	2.644666
224.944686	2245.059122	17.869261	-0.044137	2.640429
225.034091	2237.090089	17.874266	-0.044148	2.636176
224.980764	2229.092287	17.879271	-0.044133	2.631892
224.909704	2221.123396	17.884275	-0.044115	2.627616
224.728310	2213.150655	17.889280	-0.044077	2.623323
224.810587	2205.204825	17.894285	-0.044087	2.619055
224.776270	2197.239738	17.899290	-0.044076	2.614761
224.458430	2189.268616	17.904295	-0.044011	2.610439
224.777779	2181.269434	17.909299	-0.044066	2.606137
224.495197	2173.329437	17.914304	-0.044008	2.601819
224.385087	2165.379828	17.919309	-0.043983	2.597500
224.375155	2157.341401	17.924314	-0.043976	2.593133
224.209308	2149.245739	17.929319	-0.043940	2.588717
224.308675	2141.297282	17.934323	-0.043954	2.584391
224.262928	2133.356859	17.939328	-0.043940	2.580053
224.343292	2125.418521	17.944333	-0.043950	2.575717
224.223146	2117.476892	17.949338	-0.043923	2.571358
224.121447	2109.497015	17.954343	-0.043899	2.566972
224.256615	2101.544611	17.959347	-0.043919	2.562610
224.069568	2093.599964	17.964352	-0.043880	2.558223
223.872081	2085.666983	17.969357	-0.043838	2.553834
223.967873	2077.654654	17.974362	-0.043851	2.549413
223.939465	2069.677856	17.979367	-0.043841	2.544996
223.947583	2061.744587	17.984371	-0.043837	2.540598
223.533402	2053.821021	17.989376	-0.043755	2.536168
223.794180	2045.804367	17.994381	-0.043799	2.531726
223.645810	2037.842728	17.999386	-0.043766	2.527278
223.527581	2029.884907	18.004391	-0.043739	2.522827
223.511392	2021.927556	18.009395	-0.043731	2.518375
223.355016	2013.970272	18.014400	-0.043697	2.513905
223.425633	2005.964976	18.019405	-0.043705	2.509416
223.367725	1997.988564	18.024410	-0.043690	2.504927
223.464104	1990.025681	18.029415	-0.043703	2.500448
223.482498	1982.082929	18.034419	-0.043701	2.495967
223.441859	1974.075444	18.039424	-0.043689	2.491436
223.562553	1966.119184	18.044429	-0.043706	2.486939
223.341519	1958.184474	18.049434	-0.043660	2.482420
223.205727	1950.251617	18.054439	-0.043630	2.477901
223.285577	1942.280600	18.059443	-0.043640	2.473367
223.257967	1934.285665	18.064448	-0.043630	2.468803
223.032680	1926.346058	18.069453	-0.043583	2.464248
222.907328	1918.409563	18.074458	-0.043555	2.459694
222.933815	1910.437788	18.079463	-0.043555	2.455122
222.675786	1902.503759	18.084467	-0.043502	2.450542
222.459135	1894.529457	18.089472	-0.043456	2.445934
222.696173	1886.551470	18.094477	-0.043496	2.441348
222.777667	1878.582357	18.099482	-0.043506	2.436748
222.577417	1870.585417	18.104487	-0.043463	2.432101
222.601264	1862.596588	18.109491	-0.043463	2.427467
222.659855	1854.614102	18.114496	-0.043469	2.422831
222.568814	1846.702811	18.119501	-0.043447	2.418216
222.467008	1838.753323	18.124506	-0.043423	2.413569
222.452167	1830.777778	18.129511	-0.043415	2.408904
222.355187	1822.834200	18.134515	-0.043392	2.404242
222.167822	1814.905635	18.139520	-0.043353	2.399574
222.150271	1806.955904	18.144525	-0.043344	2.394896
222.035424	1798.974899	18.149530	-0.043318	2.390184
221.920608	1791.022370	18.154535	-0.043292	2.385479
221.991239	1783.057847	18.159539	-0.043300	2.380773
221.839643	1775.119635	18.164544	-0.043267	2.376055
221.690193	1767.167061	18.169549	-0.043234	2.371319
221.530407	1759.210891	18.174554	-0.043199	2.366571
221.574850	1751.236201	18.179559	-0.043203	2.361818
221.760214	1743.276249	18.184563	-0.043232	2.357076
221.533004	1735.324658	18.189568	-0.043185	2.352297
221.634037	1727.327011	18.194573	-0.043199	2.347506
222.099543	1719.321372	18.199578	-0.043281	2.342731
221.699262	1711.453387	18.204583	-0.043201	2.337958
221.558598	1703.512967	18.209587	-0.043170	2.333152
221.471797	1695.520567	18.214592	-0.043149	2.328310
221.439864	1687.585462	18.219597	-0.043138	2.323497
221.476439	1679.635638	18.224602	-0.043140	2.318671
221.385705	1671.688993	18.229607	-0.043118	2.313826
221.481249	1663.710026	18.234611	-0.043131	2.308966
221.228248	1655.769282	18.239616	-0.043079	2.304091
221.279605	1647.832489	18.244621	-0.043084	2.299233
221.293874	1639.871038	18.249626	-0.043081	2.294347
221.149994	1631.913825	18.254631	-0.043050	2.289439
220.799051	1624.013933	18.259635	-0.042979	2.284539
220.908801	1616.040876	18.264640	-0.042995	2.279622
220.966379	1608.100706	18.269645	-0.043001	2.274710
220.713923	1600.079082	18.274650	-0.042949	2.269710
220.708041	1592.111315	18.279655	-0.042943	2.264755
220.895259	1584.167948	18.284659	-0.042973	2.259820
220.542554	1576.262916	18.289664	-0.042902	2.254851
220.657166	1568.277617	18.294669	-0.042918	2.249862
220.632046	1560.334630	18.299674	-0.042909	2.244876
220.507760	1552.408255	18.304679	-0.042881	2.239881
220.484764	1544.486962	18.309683	-0.042872	2.234887
220.396469	1536.502168	18.314688	-0.042850	2.229835
220.281454	1528.569059	18.319693	-0.042824	2.224803
220.179087	1520.645309	18.324698	-0.042800	2.219766
219.967342	1512.713783	18.329703	-0.042755	2.214703
220.296432	1504.708277	18.334707	-0.042812	2.209629
220.181850	1496.771224	18.339712	-0.042786	2.204548
220.159872	1488.858704	18.344717	-0.042777	2.199479
219.993755	1480.937420	18.349722	-0.042741	2.194380
219.957209	1472.943129	18.354727	-0.042729	2.189234
219.913085	1465.003050	18.359731	-0.042716	2.184109
219.781155	1457.082258	18.364736	-0.042686	2.178977
219.703819	1449.140201	18.369741	-0.042667	2.173824
219.803827	1441.158176	18.374746	-0.042681	2.168650
219.672907	1433.226092	18.379751	-0.042651	2.163474
219.905134	1425.290176	18.384755	-0.042690	2.158317
219.612053	1417.370848	18.389760	-0.042630	2.153109
219.387293	1409.437802	18.394765	-0.042583	2.147886
219.476859	1401.482738	18.399770	-0.042595	2.142665
219.512981	1393.542575	18.404775	-0.042597	2.137437
219.365177	1385.621299	18.409779	-0.042564	2.132191
219.255157	1377.675798	18.414784	-0.042539	2.126919
219.149376	1369.761660	18.419789	-0.042514	2.121655
219.178706	1361.830638	18.424794	-0.042515	2.116380
219.168979	1353.816090	18.429799	-0.042508	2.111032
219.146774	1345.863732	18.434803	-0.042499	2.105711
219.388830	1337.911818	18.439808	-0.042539	2.100403
219.060932	1330.044557	18.444813	-0.042473	2.095082
218.748722	1322.133928	18.449818	-0.042410	2.089720
218.921077	1314.163245	18.454823	-0.042437	2.084351
218.810884	1306.267178	18.459827	-0.042412	2.078992
218.708068	1298.329404	18.464832	-0.042388	2.073590
218.706750	1290.374895	18.469837	-0.042383	2.068173
218.375674	1282.487780	18.474842	-0.042316	2.062755
218.513012	1274.521670	18.479847	-0.042337	2.057316
218.535485	1266.603770	18.484851	-0.042336	2.051884
218.554881	1258.644276	18.489856	-0.042335	2.046408
218.439871	1250.747245	18.494861	-0.042309	2.040947
218.208926	1242.859624	18.499866	-0.042261	2.035466
218.340033	1234.855158	18.504871	-0.042280	2.029927
218.336168	1226.932200	18.509875	-0.042274	2.024414
218.151384	1219.029795	18.514880	-0.042235	2.018883
218.297388	1211.080214	18.519885	-0.042257	2.013338
218.229183	1203.156540	18.524890	-0.042240	2.007773
218.150702	1195.241978	18.529895	-0.042220	2.002198
218.050734	1187.358871	18.534899	-0.042197	1.996627
218.016855	1179.395657	18.539904	-0.042186	1.990991
217.884660	1171.483461	18.544909	-0.042156	1.985365
217.842470	1163.574665	18.549914	-0.042143	1.979735
217.827199	1155.654423	18.554919	-0.042135	1.974083
217.712652	1147.737246	18.559923	-0.042109	1.968407
217.432024	1139.845646	18.564928	-0.042052	1.962715
217.666880	1131.899522	18.569933	-0.042091	1.957022
217.535340	1123.964703	18.574938	-0.042061	1.951282
217.163791	1116.054024	18.579943	-0.041987	1.945516
217.311530	1108.132822	18.584947	-0.042010	1.939781
217.325640	1100.194204	18.589952	-0.042008	1.934003
217.169319	1092.288517	18.594957	-0.041974	1.928212
217.183560	1084.372430	18.599962	-0.041971	1.922415
217.240984	1076.461136	18.604967	-0.041977	1.916609
217.319119	1068.523649	18.609971	-0.041987	1.910768
217.181483	1060.608854	18.614976	-0.041956	1.904902
217.045657	1052.745782	18.619981	-0.041926	1.899056
216.946830	1044.843549	18.624986	-0.041903	1.893167
216.979771	1036.898920	18.629991	-0.041904	1.887244
216.916201	1029.020514	18.634995	-0.041887	1.881340
216.598356	1021.155584	18.640000	-0.041823	1.875398
216.655635	1013.203741	18.645005	-0.041829	1.869415
216.629790	1005.288111	18.650010	-0.041819	1.863431
216.518138	997.397244	18.655015	-0.041794	1.857436
216.666782	989.471960	18.660019	-0.041816	1.851426
216.420082	981.579764	18.665024	-0.041765	1.845376
216.464763	973.694132	18.670029	-0.041769	1.839345
216.399567	965.801261	18.675034	-0.041752	1.833275
216.134948	957.901542	18.680039	-0.041698	1.827156
216.407885	949.958931	18.685043	-0.041744	1.821048
216.290242	942.088091	18.690048	-0.041717	1.814928
216.188384	934.198381	18.695053	-0.041693	1.808774
216.188871	926.296992	18.700058	-0.041688	1.802603
216.122266	918.417500	18.705063	-0.041671	1.796419
216.005417	910.484380	18.710067	-0.041644	1.790166
215.779110	902.596825	18.715072	-0.041597	1.783913
215.980810	894.692585	18.720077	-0.041630	1.777678
215.826743	886.816519	18.725082	-0.041596	1.771399
215.639314	878.936556	18.730087	-0.041556	1.765090
215.698886	871.062895	18.735091	-0.041563	1.758795
215.609804	863.175567	18.740096	-0.041541	1.752448
215.547541	855.275744	18.745101	-0.041525	1.746070
215.421675	847.418987	18.750106	-0.041496	1.739696
215.376283	839.526870	18.755111	-0.041483	1.733281
215.326961	831.642031	18.760115	-0.041469	1.726846
215.178871	823.780009	18.765120	-0.041437	1.720394
215.270520	815.895999	18.770125	-0.041449	1.713930
215.262903	807.997322	18.775130	-0.041442	1.707417
215.035680	800.139093	18.780135	-0.041395	1.700883
215.067005	792.274517	18.785139	-0.041396	1.694353
215.020819	784.377148	18.790144	-0.041383	1.687760
214.935436	776.525947	18.795149	-0.041362	1.681175
214.839557	768.679398	18.800154	-0.041339	1.674567
214.887482	760.772739	18.805159	-0.041343	1.667900
214.928660	752.907476	18.810163	-0.041346	1.661241
214.626985	745.085702	18.815168	-0.041285	1.654546
214.517319	737.218748	18.820173	-0.041260	1.647811
214.376784	729.383660	18.825178	-0.041229	1.641072
214.268043	721.521861	18.830183	-0.041204	1.634286
214.338286	713.593550	18.835187	-0.041212	1.627439
214.251508	705.736682	18.840192	-0.041191	1.620603
214.253463	697.894839	18.845197	-0.041186	1.613764
214.020373	690.058782	18.850202	-0.041138	1.606867
214.126279	682.180852	18.855207	-0.041153	1.599952
214.140521	674.354353	18.860211	-0.041151	1.593040
213.985712	666.503113	18.865216	-0.041117	1.586051
213.924181	658.671188	18.870221	-0.041101	1.579061
213.773068	650.849413	18.875226	-0.041068	1.572037
213.684401	642.993190	18.880231	-0.041046	1.564959
213.501415	635.198469	18.885235	-0.041007	1.557891
213.587768	627.315658	18.890240	-0.041018	1.550751
213.625696	619.465720	18.895245	-0.041021	1.543600
213.332506	611.674825	18.900250	-0.040961	1.536420
213.263109	603.837181	18.905255	-0.040943	1.529198
213.390144	595.992812	18.910259	-0.040962	1.521964
213.240955	588.190091	18.915264	-0.040930	1.514693
213.247884	580.349585	18.920269	-0.040926	1.507375
213.285803	572.524729	18.925274	-0.040928	1.500040
212.986378	564.748865	18.930279	-0.040868	1.492664
212.980765	556.921049	18.935283	-0.040862	1.485248
212.751361	549.147147	18.940288	-0.040814	1.477811
212.702573	541.297184	18.945293	-0.040800	1.470291
212.783980	533.457702	18.950298	-0.040811	1.462764
212.684790	525.658906	18.955303	-0.040787	1.455208
212.823914	517.833696	18.960307	-0.040808	1.447625
212.419194	510.103906	18.965312	-0.040728	1.440008
212.439306	502.302854	18.970317	-0.040727	1.432350
212.399032	494.497864	18.975322	-0.040715	1.424636
212.273546	486.727215	18.980327	-0.040687	1.416900
212.274562	478.936626	18.985331	-0.040682	1.409123
212.272597	471.140726	18.990336	-0.040677	1.401297
212.020644	463.409677	18.995341	-0.040625	1.393451
211.896612	455.620177	19.000346	-0.040597	1.385522
211.794661	447.854249	19.005351	-0.040573	1.377575
211.897658	440.058858	19.010355	-0.040588	1.369587
211.620937	432.323128	19.015360	-0.040531	1.361549
211.677137	424.555913	19.020365	-0.040537	1.353488
211.582047	416.798385	19.025370	-0.040514	1.345362
211.460467	409.060622	19.030375	-0.040487	1.337202
211.285592	401.328951	19.035379	-0.040450	1.328990
211.364069	393.555577	19.040384	-0.040460	1.320727
211.472155	385.754450	19.045389	-0.040475	1.312388
211.221741	377.972903	19.050394	-0.040423	1.303952
210.952069	370.285290	19.055399	-0.040368	1.295559
211.087550	362.535442	19.060403	-0.040389	1.287118
210.873044	354.850325	19.065408	-0.040344	1.278628
210.870581	347.129399	19.070413	-0.040339	1.270080
210.680234	339.446633	19.075418	-0.040299	1.261482
210.609050	331.745325	19.080423	-0.040281	1.252827
210.474050	324.065350	19.085427	-0.040251	1.244124
210.568511	316.347419	19.090432	-0.040264	1.235360
210.389666	308.660640	19.095437	-0.040225	1.226516
210.278410	300.993248	19.100442	-0.040200	1.217643
210.035192	293.333924	19.105447	-0.040150	1.208689
210.261420	285.630142	19.110451	-0.040187	1.199709
210.127974	277.981480	19.115456	-0.040158	1.190654
209.758448	270.372489	19.120461	-0.040084	1.181529
209.801208	262.706287	19.125466	-0.040087	1.172349
209.596714	255.079851	19.130471	-0.040045	1.163093
209.538989	247.447748	19.135475	-0.040029	1.153787
209.451327	239.783486	19.140480	-0.040008	1.144359
209.378108	232.165667	19.145485	-0.039990	1.134913
209.308000	224.550009	19.150490	-0.039972	1.125392
209.156174	216.965463	19.155495	-0.039939	1.115811
209.213118	209.348696	19.160499	-0.039945	1.106151
209.063485	201.777761	19.165504	-0.039912	1.096420
208.930851	194.204116	19.170509	-0.039883	1.086601
209.106650	186.611974	19.175514	-0.039911	1.076739
208.777648	179.079020	19.180519	-0.039845	1.066748
208.789173	171.527070	19.185523	-0.039843	1.056716
208.639081	163.993607	19.190528	-0.039810	1.046575
208.698587	156.460713	19.195533	-0.039816	1.036385
208.627438	148.944029	19.200538	-0.039798	1.026085
208.307619	141.482267	19.205543	-0.039734	1.015697
208.084714	134.022101	19.210547	-0.039688	1.005227
208.115011	126.522195	19.215552	-0.039689	0.994652
207.876547	119.050374	19.220557	-0.039640	0.983938
207.609035	111.628798	19.225562	-0.039586	0.973171
207.639816	104.159274	19.230567	-0.039587	0.962289
207.652094	96.729069	19.235571	-0.039585	0.951336
207.248280	89.376417	19.240576	-0.039505	0.940263
206.984813	82.008379	19.245581	-0.039451	0.929071
207.139674	74.597348	19.250586	-0.039476	0.917790
206.864916	67.251270	19.255591	-0.039420	0.906352
206.803560	60.147655	19.260595	-0.039404	0.895209