Thu Mar 11 19:19:20 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.593949	-0.007571	0.000000	-0.000006	0.724464

0.598059	-0.111915	0.005005	-0.000006	0.724262
0.655118	-0.123868	0.010010	-0.000017	0.724259
0.712581	-0.132665	0.015014	-0.000028	0.724262
0.620250	-0.120533	0.020019	-0.000011	0.724254
0.685859	-0.126794	0.025024	-0.000024	0.724265
0.555633	-0.105325	0.030029	0.000000	0.724262
0.568797	-0.110301	0.035034	-0.000002	0.724257
0.728062	-0.134432	0.040038	-0.000032	0.724266
0.744107	-0.142751	0.045043	-0.000035	0.724256
0.542620	-0.102974	0.050048	0.000002	0.724264
0.571067	-0.108798	0.055053	-0.000004	0.724263
0.599554	-0.116422	0.060058	-0.000009	0.724258
0.422379	-0.080495	0.065062	0.000024	0.724267
0.523441	-0.102714	0.070067	0.000005	0.724259
0.533282	-0.180911	0.075072	0.000003	0.724110
0.545444	-0.263171	0.080077	0.000000	0.723953
0.532851	-0.261409	0.085082	0.000002	0.723953
0.648290	-0.280130	0.090086	-0.000019	0.723957
0.403302	-0.242769	0.095091	0.000026	0.723945
0.421542	-0.241795	0.100096	0.000023	0.723953
0.680564	-0.287793	0.105101	-0.000026	0.723954
0.383600	-0.380839	0.110106	0.000029	0.723669
0.498360	-0.418000	0.115110	0.000008	0.723636
0.374485	-0.399730	0.120115	0.000031	0.723629
0.516484	-0.422624	0.125120	0.000004	0.723634
0.461199	-0.411946	0.130125	0.000014	0.723636
0.406776	-0.509572	0.135130	0.000024	0.723426
0.588554	-0.582307	0.140134	-0.000010	0.723348
0.370013	-0.548455	0.145139	0.000030	0.723338
0.517475	-0.572601	0.150144	0.000003	0.723343
0.556629	-0.650826	0.155149	-0.000005	0.723203
0.520276	-0.745557	0.160154	0.000002	0.723005
0.602734	-0.757614	0.165158	-0.000014	0.723011
0.669885	-0.773233	0.170163	-0.000026	0.723004
0.608744	-0.882855	0.175168	-0.000015	0.722768
0.368278	-0.878187	0.180173	0.000030	0.722693
0.424551	-0.890435	0.185178	0.000019	0.722689
0.671576	-0.990895	0.190182	-0.000027	0.722579
0.629422	-1.092060	0.195187	-0.000020	0.722366
0.711943	-1.104290	0.200192	-0.000035	0.722371
0.663481	-1.155769	0.205197	-0.000026	0.722254
0.502316	-1.219639	0.210202	0.000004	0.722072
0.419998	-1.201566	0.215206	0.000019	0.722079
0.261534	-1.257829	0.220211	0.000048	0.721914
0.553108	-1.395637	0.225216	-0.000006	0.721746
0.534226	-1.392317	0.230221	-0.000003	0.721746
0.360371	-1.483524	0.235226	0.000029	0.721506
0.587873	-1.554492	0.240230	-0.000013	0.721447
0.439089	-1.565004	0.245235	0.000014	0.721374
0.365509	-1.677972	0.250240	0.000028	0.721127
0.301732	-1.667887	0.255245	0.000039	0.721125
0.267486	-1.752822	0.260250	0.000045	0.720946
0.202628	-1.774444	0.265254	0.000057	0.720881
0.282141	-1.842320	0.270259	0.000042	0.720776
0.252291	-1.954841	0.275264	0.000048	0.720544
0.273739	-1.958306	0.280269	0.000044	0.720545
0.255576	-2.119249	0.285274	0.000047	0.720223
0.335102	-2.129133	0.290278	0.000032	0.720231
0.270539	-2.255592	0.295283	0.000044	0.719960
0.035249	-2.243012	0.300288	0.000087	0.719903
-0.260672	-2.286854	0.305293	0.000142	0.719713
-0.055036	-2.378531	0.310298	0.000104	0.719605
0.001475	-2.468984	0.315302	0.000093	0.719447
-0.144360	-2.534110	0.320307	0.000120	0.719268
0.028966	-2.627401	0.325312	0.000088	0.719145
-0.045949	-2.705989	0.330317	0.000102	0.718964
-0.141881	-2.761348	0.335322	0.000119	0.718822
-3.897875	-2.180406	0.340326	0.000818	0.718648
-5.079648	-1.976021	0.345331	0.001038	0.718637
-6.003948	-1.806855	0.350336	0.001209	0.718646
-4.837088	-2.083919	0.355341	0.000992	0.718510
-6.308973	-1.901824	0.360346	0.001266	0.718352
-6.137294	-1.926634	0.365350	0.001234	0.718364
-6.172136	-1.925570	0.370355	0.001240	0.718354
-6.486109	-1.867320	0.375360	0.001298	0.718359
-6.224191	-1.915356	0.380365	0.001249	0.718357
-6.114516	-2.029513	0.385370	0.001229	0.718170
-7.367536	-1.881850	0.390374	0.001462	0.718021
-7.749803	-1.817521	0.395379	0.001533	0.718014
-7.498818	-1.860489	0.400384	0.001486	0.718018
-7.273173	-1.900524	0.405389	0.001444	0.718019
-7.499683	-1.862831	0.410394	0.001486	0.718014
-7.231448	-1.905078	0.415398	0.001435	0.718025
-7.333556	-2.000941	0.420403	0.001454	0.717801
-8.351975	-1.869705	0.425408	0.001644	0.717702
-8.284051	-1.880740	0.430413	0.001631	0.717704
-8.249489	-1.888519	0.435418	0.001624	0.717701
-8.321117	-1.871460	0.440422	0.001637	0.717710
-8.323143	-1.874893	0.445427	0.001637	0.717703
-8.090976	-1.915460	0.450432	0.001594	0.717705
-8.555935	-1.970955	0.455437	0.001680	0.717432
-9.676499	-1.799312	0.460442	0.001889	0.717377
-9.315998	-1.858001	0.465446	0.001821	0.717389
-9.124849	-1.896671	0.470451	0.001786	0.717380
-9.351567	-1.856410	0.475456	0.001828	0.717380
-9.474975	-1.831155	0.480461	0.001850	0.717387
-9.355232	-1.856671	0.485466	0.001828	0.717379
-9.149590	-1.943548	0.490470	0.001789	0.717280
-10.290739	-1.840478	0.495475	0.002002	0.717082
-10.001751	-1.888525	0.500480	0.001948	0.717090
-10.084429	-1.874077	0.505485	0.001963	0.717089
-10.325729	-1.834887	0.510490	0.002008	0.717082
-10.193224	-1.854114	0.515494	0.001983	0.717091
-10.210759	-1.854742	0.520499	0.001986	0.717084
-10.315954	-1.845043	0.525504	0.002005	0.717067
-10.853403	-1.905397	0.530509	0.002105	0.716758
-10.906303	-1.899330	0.535514	0.002115	0.716752
-10.856079	-1.901102	0.540518	0.002105	0.716767
-11.268106	-1.833352	0.545523	0.002182	0.716756
-11.130713	-1.857474	0.550528	0.002156	0.716757
-10.665798	-1.940095	0.555533	0.002069	0.716758
-11.245660	-1.839924	0.560538	0.002177	0.716752
-11.709450	-1.900790	0.565542	0.002263	0.716468
-11.826711	-1.890431	0.570547	0.002285	0.716448
-11.934046	-1.870014	0.575552	0.002304	0.716451
-11.837935	-1.886153	0.580557	0.002286	0.716453
-12.003050	-1.861001	0.585562	0.002317	0.716445
-11.729949	-1.904292	0.590566	0.002266	0.716456
-12.257829	-1.816571	0.595571	0.002364	0.716444
-12.520940	-1.888845	0.600576	0.002413	0.716209
-12.898033	-1.859699	0.605581	0.002482	0.716134
-13.090161	-1.829339	0.610586	0.002518	0.716126
-13.026814	-1.836175	0.615590	0.002506	0.716136
-13.124177	-1.823090	0.620595	0.002524	0.716128
-12.860991	-1.867573	0.625600	0.002475	0.716133
-12.772725	-1.882119	0.630605	0.002458	0.716135
-12.822442	-1.910891	0.635610	0.002467	0.716061
-13.371155	-1.900242	0.640614	0.002569	0.715889
-13.848887	-1.820343	0.645619	0.002658	0.715879
-14.241768	-1.748311	0.650624	0.002731	0.715884
-13.449734	-1.887832	0.655629	0.002583	0.715887
-13.585826	-1.866192	0.660634	0.002608	0.715882
-13.839458	-1.818966	0.665638	0.002655	0.715887
-13.539413	-1.929209	0.670643	0.002599	0.715775
-14.477601	-1.878193	0.675648	0.002774	0.715545
-14.379036	-1.893591	0.680653	0.002755	0.715550
-14.819763	-1.819177	0.685658	0.002837	0.715542
-14.699654	-1.836247	0.690662	0.002814	0.715551
-14.580584	-1.861557	0.695667	0.002792	0.715543
-14.628520	-1.851604	0.700672	0.002801	0.715546
-14.271426	-1.976431	0.705677	0.002734	0.715425
-15.676190	-1.824449	0.710682	0.002995	0.715231
-15.613568	-1.832461	0.715686	0.002983	0.715237
-15.586736	-1.839960	0.720691	0.002978	0.715232
-15.655587	-1.827384	0.725696	0.002991	0.715233
-15.617282	-1.834330	0.730701	0.002984	0.715234
-16.009199	-1.769001	0.735706	0.003056	0.715225
-15.244298	-1.901847	0.740710	0.002914	0.715232
-16.019110	-1.926446	0.745715	0.003058	0.714910
-16.821196	-1.784305	0.750720	0.003207	0.714909
-16.510740	-1.836668	0.755725	0.003149	0.714915
-16.240165	-1.889831	0.760730	0.003098	0.714906
-16.560115	-1.829571	0.765734	0.003158	0.714913
-16.638789	-1.819217	0.770739	0.003172	0.714906
-16.433290	-1.853157	0.775744	0.003134	0.714911
-16.678860	-1.908666	0.780749	0.003179	0.714715
-17.982341	-1.732394	0.785754	0.003422	0.714604
-17.175013	-1.872140	0.790758	0.003271	0.714613
-17.339659	-1.845445	0.795763	0.003302	0.714608
-17.635462	-1.792004	0.800768	0.003356	0.714610
-17.033016	-1.896900	0.805773	0.003244	0.714615
-17.198924	-1.872536	0.810778	0.003275	0.714605
-17.629592	-1.876590	0.815782	0.003355	0.714445
-18.611966	-1.786617	0.820787	0.003537	0.714276
-17.921557	-1.907777	0.825792	0.003409	0.714281
-18.439319	-1.815105	0.830797	0.003505	0.714282
-18.850667	-1.744889	0.835802	0.003581	0.714276
-18.060157	-1.883019	0.840806	0.003434	0.714282
-18.200639	-1.860942	0.845811	0.003460	0.714276
-18.693808	-1.771827	0.850816	0.003551	0.714279
-18.883704	-1.885276	0.855821	0.003587	0.713987
-19.115045	-1.854512	0.860826	0.003629	0.713967
-19.292994	-1.819238	0.865830	0.003662	0.713974
-19.394228	-1.804388	0.870835	0.003681	0.713968
-19.433230	-1.796462	0.875840	0.003688	0.713971
-19.401136	-1.800927	0.880845	0.003682	0.713974
-19.465264	-1.793316	0.885850	0.003694	0.713966
-19.252028	-1.894264	0.890854	0.003654	0.713842
-19.947064	-1.867218	0.895859	0.003783	0.713650
-20.137095	-1.832463	0.900864	0.003818	0.713652
-20.208071	-1.817349	0.905869	0.003831	0.713657
-20.203533	-1.820910	0.910874	0.003830	0.713652
-20.028742	-1.847345	0.915878	0.003797	0.713662
-20.178184	-1.824925	0.920883	0.003825	0.713654
-20.211185	-1.886840	0.925888	0.003831	0.713519
-20.801124	-1.861323	0.930893	0.003940	0.713362
-21.422844	-1.755775	0.935898	0.004056	0.713352
-21.249123	-1.782180	0.940902	0.004023	0.713361
-21.190497	-1.795612	0.945907	0.004012	0.713355
-21.237834	-1.786790	0.950912	0.004021	0.713357
-20.932842	-1.837722	0.955917	0.003964	0.713364
-21.080868	-1.817631	0.960922	0.003991	0.713352
-21.550132	-1.892948	0.965926	0.004078	0.713036
-22.318815	-1.765758	0.970931	0.004221	0.713017
-22.418865	-1.745035	0.975936	0.004240	0.713023
-21.972725	-1.822569	0.980941	0.004156	0.713027
-22.369742	-1.756150	0.985946	0.004230	0.713019
-22.319989	-1.760901	0.990950	0.004221	0.713028
-21.838344	-1.850645	0.995955	0.004131	0.713020
-22.356936	-1.789232	1.000960	0.004227	0.712959
-22.893849	-1.817238	1.005965	0.004327	0.712713
-22.833214	-1.831340	1.010970	0.004315	0.712707
-22.894474	-1.817019	1.015974	0.004327	0.712714
-22.957638	-1.809885	1.020979	0.004338	0.712706
-23.044616	-1.794471	1.025984	0.004354	0.712707
-22.696668	-1.852278	1.030989	0.004289	0.712715
-23.283445	-1.753220	1.035994	0.004398	0.712705
-23.495639	-1.861020	1.040998	0.004438	0.712415
-23.977715	-1.788137	1.046003	0.004527	0.712390
-24.250452	-1.741857	1.051008	0.004578	0.712386
-23.929789	-1.796020	1.056013	0.004518	0.712392
-23.863716	-1.811521	1.061018	0.004505	0.712385
-23.989835	-1.785606	1.066022	0.004528	0.712392
-23.990409	-1.789348	1.071027	0.004528	0.712385
-24.092095	-1.827889	1.076032	0.004547	0.712272
-24.619615	-1.823406	1.081037	0.004645	0.712094
-24.618427	-1.828283	1.086042	0.004645	0.712086
-24.960096	-1.763060	1.091046	0.004708	0.712095
-24.849344	-1.785306	1.096051	0.004687	0.712090
-24.903890	-1.776023	1.101056	0.004697	0.712090
-24.992745	-1.758237	1.106061	0.004713	0.712094
-24.866975	-1.800274	1.111066	0.004690	0.712055
-25.218625	-1.882889	1.116070	0.004755	0.711766
-25.568636	-1.822992	1.121075	0.004820	0.711761
-26.046915	-1.736755	1.126080	0.004909	0.711764
-25.274449	-1.872997	1.131085	0.004765	0.711767
-25.497993	-1.837670	1.136090	0.004806	0.711758
-26.013511	-1.741470	1.141094	0.004902	0.711768
-25.655124	-1.826162	1.146099	0.004835	0.711726
-26.515972	-1.808461	1.151104	0.004995	0.711456
-26.544656	-1.802377	1.156109	0.005000	0.711459
-26.762761	-1.766921	1.161114	0.005041	0.711452
-26.368213	-1.833946	1.166118	0.004967	0.711459
-26.387700	-1.833648	1.171123	0.004971	0.711453
-26.677114	-1.782081	1.176128	0.005024	0.711454
-26.262740	-1.869738	1.181133	0.004947	0.711426
-27.111879	-1.865756	1.186138	0.005105	0.711133
-27.406801	-1.807066	1.191142	0.005159	0.711145
-27.747610	-1.750682	1.196147	0.005223	0.711137
-27.632868	-1.769608	1.201152	0.005201	0.711141
-27.633239	-1.768805	1.206157	0.005201	0.711142
-27.869105	-1.730925	1.211162	0.005245	0.711135
-27.365857	-1.815797	1.216166	0.005151	0.711145
-27.589180	-1.866070	1.221171	0.005192	0.710965
-28.753637	-1.705291	1.226176	0.005409	0.710872
-28.075803	-1.822921	1.231181	0.005282	0.710879
-28.215119	-1.804433	1.236186	0.005308	0.710867
-28.647428	-1.724156	1.241190	0.005388	0.710874
-28.490308	-1.754975	1.246195	0.005359	0.710868
-28.440580	-1.762787	1.251200	0.005349	0.710871
-28.543750	-1.825600	1.256205	0.005368	0.710709
-29.623057	-1.724562	1.261210	0.005569	0.710527
-28.898151	-1.848553	1.266214	0.005434	0.710538
-28.986058	-1.836292	1.271219	0.005450	0.710532
-29.750515	-1.701161	1.276224	0.005592	0.710530
-29.014806	-1.827898	1.281229	0.005455	0.710539
-29.299944	-1.783694	1.286234	0.005508	0.710526
-29.598887	-1.791340	1.291238	0.005563	0.710405
-30.563078	-1.713818	1.296243	0.005743	0.710217
-30.017431	-1.812509	1.301248	0.005641	0.710214
-30.246389	-1.768626	1.306253	0.005683	0.710221
-30.302743	-1.763042	1.311258	0.005694	0.710212
-30.191954	-1.777948	1.316262	0.005673	0.710223
-30.562645	-1.714549	1.321267	0.005742	0.710218
-30.620249	-1.705226	1.326272	0.005752	0.710216
-30.136396	-1.897057	1.331277	0.005662	0.710005
-31.170847	-1.772094	1.336282	0.005854	0.709887
-31.099758	-1.780826	1.341286	0.005841	0.709895
-30.771659	-1.840280	1.346291	0.005779	0.709894
-31.055857	-1.789442	1.351296	0.005832	0.709895
-31.294659	-1.744548	1.356301	0.005876	0.709900
-31.353836	-1.740683	1.361306	0.005887	0.709887
-31.545666	-1.805647	1.366310	0.005923	0.709689
-32.016909	-1.770177	1.371315	0.006010	0.709592
-32.205462	-1.736736	1.376320	0.006045	0.709592
-31.976004	-1.774514	1.381325	0.006002	0.709599
-32.169652	-1.744105	1.386330	0.006038	0.709591
-32.203290	-1.734253	1.391334	0.006044	0.709599
-32.129568	-1.748490	1.396339	0.006030	0.709597
-32.174887	-1.786307	1.401344	0.006038	0.709506
-33.129361	-1.733315	1.406349	0.006216	0.709272
-33.011391	-1.760470	1.411354	0.006194	0.709260
-33.158552	-1.730231	1.416358	0.006221	0.709269
-32.958570	-1.766151	1.421363	0.006183	0.709269
-33.052818	-1.751856	1.426368	0.006201	0.709264
-32.899264	-1.774275	1.431373	0.006172	0.709274
-33.153712	-1.734277	1.436378	0.006219	0.709264
-33.426422	-1.810623	1.441382	0.006270	0.709014
-34.213880	-1.700148	1.446387	0.006416	0.708955
-33.998813	-1.738446	1.451392	0.006376	0.708955
-33.587997	-1.809720	1.456397	0.006299	0.708960
-34.048038	-1.731088	1.461402	0.006385	0.708953
-33.866915	-1.760646	1.466406	0.006351	0.708959
-33.478356	-1.830605	1.471411	0.006278	0.708958
-34.521933	-1.756137	1.476416	0.006472	0.708735
-35.047260	-1.708383	1.481421	0.006570	0.708644
-34.694099	-1.776282	1.486426	0.006504	0.708634
-34.758263	-1.759513	1.491430	0.006516	0.708645
-34.897932	-1.737432	1.496435	0.006541	0.708640
-34.586760	-1.795314	1.501440	0.006483	0.708636
-34.481776	-1.809745	1.506445	0.006464	0.708645
-34.904772	-1.805236	1.511450	0.006542	0.708503
-35.643856	-1.749281	1.516454	0.006679	0.708352
-35.041931	-1.854895	1.521459	0.006567	0.708355
-35.583376	-1.760501	1.526464	0.006668	0.708352
-35.410464	-1.786107	1.531469	0.006635	0.708362
-35.138872	-1.840596	1.536474	0.006585	0.708351
-35.430079	-1.806500	1.541478	0.006639	0.708315
-36.394601	-1.785059	1.546483	0.006818	0.708014
-36.366106	-1.791273	1.551488	0.006813	0.708012
-36.377083	-1.785118	1.556493	0.006814	0.708021
-36.686523	-1.735148	1.561498	0.006872	0.708011
-36.431799	-1.776001	1.566502	0.006824	0.708021
-36.321489	-1.799289	1.571507	0.006803	0.708014
-36.477880	-1.772511	1.576512	0.006832	0.708012
-36.777461	-1.871892	1.581517	0.006888	0.707706
-37.317175	-1.778968	1.586522	0.006988	0.707700
-37.537221	-1.736251	1.591526	0.007029	0.707707
-37.236288	-1.791608	1.596531	0.006973	0.707704
-37.341160	-1.775918	1.601536	0.006992	0.707699
-37.162060	-1.803800	1.606541	0.006958	0.707707
-37.539469	-1.742724	1.611546	0.007028	0.707695
-37.906854	-1.833913	1.616550	0.007097	0.707381
-37.888480	-1.839490	1.621555	0.007093	0.707377
-38.416090	-1.747669	1.626560	0.007191	0.707373
-38.348507	-1.755677	1.631565	0.007178	0.707381
-38.341804	-1.760612	1.636570	0.007177	0.707374
-38.276675	-1.768338	1.641574	0.007164	0.707382
-38.210344	-1.780751	1.646579	0.007152	0.707382
-38.653255	-1.831928	1.651584	0.007234	0.707121
-38.853337	-1.811200	1.656589	0.007271	0.707091
-39.046840	-1.782780	1.661594	0.007307	0.707080
-38.744395	-1.832926	1.666598	0.007251	0.707088
-39.050803	-1.779326	1.671603	0.007307	0.707086
-39.343066	-1.729959	1.676608	0.007362	0.707081
-39.026128	-1.794779	1.681613	0.007302	0.707065
-39.703050	-1.832665	1.686618	0.007428	0.706747
-39.733169	-1.823417	1.691622	0.007434	0.706755
-40.302832	-1.722696	1.696627	0.007539	0.706753
-40.119288	-1.758062	1.701632	0.007505	0.706749
-39.753049	-1.818805	1.706637	0.007437	0.706758
-40.387187	-1.711332	1.711642	0.007554	0.706747
-40.151553	-1.749883	1.716646	0.007510	0.706755
-39.909204	-1.908753	1.721651	0.007465	0.706523
-40.959202	-1.762454	1.726656	0.007660	0.706441
-40.926238	-1.764764	1.731661	0.007654	0.706449
-40.914040	-1.772460	1.736666	0.007652	0.706438
-40.827934	-1.783427	1.741670	0.007635	0.706447
-40.934364	-1.766210	1.746675	0.007655	0.706444
-40.799500	-1.792277	1.751680	0.007630	0.706440
-41.141117	-1.859538	1.756685	0.007693	0.706183
-41.944339	-1.746490	1.761690	0.007842	0.706123
-42.080311	-1.718027	1.766694	0.007867	0.706132
-41.440231	-1.833882	1.771699	0.007748	0.706129
-41.657319	-1.797054	1.776704	0.007788	0.706125
-41.604320	-1.802975	1.781709	0.007778	0.706133
-41.398939	-1.842505	1.786714	0.007740	0.706127
-42.078685	-1.846171	1.791718	0.007866	0.705877
-42.668080	-1.747707	1.796723	0.007976	0.705864
-42.851988	-1.716599	1.801728	0.008010	0.705861
-42.236330	-1.821699	1.806733	0.007895	0.705871
-42.582199	-1.765560	1.811738	0.007959	0.705860
-42.829992	-1.720192	1.816742	0.008005	0.705863
-42.419428	-1.796182	1.821747	0.007928	0.705858
-43.229605	-1.821617	1.826752	0.008079	0.705516
-43.480579	-1.770445	1.831757	0.008125	0.705530
-43.803536	-1.716370	1.836762	0.008185	0.705523
-43.482465	-1.771945	1.841766	0.008125	0.705527
-43.517154	-1.765846	1.846771	0.008132	0.705527
-43.731145	-1.731739	1.851776	0.008171	0.705519
-43.082866	-1.842582	1.856781	0.008050	0.705529
-43.909257	-1.831621	1.861786	0.008204	0.705255
-44.840937	-1.686240	1.866790	0.008377	0.705214
-44.446725	-1.756679	1.871795	0.008304	0.705214
-44.034776	-1.835475	1.876800	0.008227	0.705203
-44.611446	-1.727328	1.881805	0.008334	0.705215
-44.638070	-1.727862	1.886810	0.008339	0.705204
-44.159523	-1.808916	1.891814	0.008249	0.705213
-44.391955	-1.865329	1.896819	0.008292	0.705017
-45.883950	-1.665350	1.901824	0.008570	0.704884
-45.037455	-1.810764	1.906829	0.008412	0.704896
-45.218674	-1.783541	1.911834	0.008446	0.704886
-45.529806	-1.725639	1.916838	0.008503	0.704891
-45.064391	-1.808580	1.921843	0.008417	0.704892
-45.334063	-1.763340	1.926848	0.008467	0.704886
-45.641304	-1.784246	1.931853	0.008524	0.704734
-46.496610	-1.704094	1.936858	0.008683	0.704589
-45.962582	-1.797410	1.941862	0.008583	0.704593
-45.857657	-1.816743	1.946867	0.008563	0.704592
-46.586915	-1.690380	1.951872	0.008699	0.704585
-46.082373	-1.776192	1.956877	0.008605	0.704594
-46.114369	-1.774950	1.961882	0.008610	0.704586
-46.384100	-1.778188	1.966886	0.008660	0.704483
-47.020450	-1.776070	1.971891	0.008779	0.704259
-46.714718	-1.832558	1.976896	0.008722	0.704255
-46.976698	-1.781484	1.981901	0.008770	0.704264
-47.344948	-1.720949	1.986906	0.008838	0.704254
-46.655868	-1.841524	1.991910	0.008710	0.704259
-46.931674	-1.793405	1.996915	0.008761	0.704258
-47.468780	-1.800897	2.001920	0.008861	0.704050

-47.802884	-1.791836	2.011917	0.008923	0.703949
-47.936951	-1.768490	2.021914	0.008947	0.703948
-48.130721	-1.735081	2.031910	0.008983	0.703947
-47.824980	-1.786970	2.041907	0.008926	0.703953
-48.005157	-1.755907	2.051904	0.008959	0.703952
-47.885689	-1.778809	2.061901	0.008936	0.703949
-48.003909	-1.758289	2.071898	0.008958	0.703949
-48.012290	-1.756034	2.081894	0.008959	0.703951
-47.835373	-1.788520	2.091891	0.008925	0.703950
-48.010321	-1.757226	2.101888	0.008958	0.703951
-47.887040	-1.764883	2.111885	0.008934	0.703981
-47.246540	-1.741348	2.121882	0.008814	0.704259
-47.070536	-1.771501	2.131878	0.008781	0.704263
-46.816482	-1.816653	2.141875	0.008734	0.704264
-47.147044	-1.759245	2.151872	0.008795	0.704262
-46.848301	-1.814652	2.161869	0.008739	0.704258
-47.092466	-1.714573	2.171866	0.008784	0.704373
-46.110159	-1.781602	2.181862	0.008600	0.704591
-46.022934	-1.796584	2.191859	0.008584	0.704593
-46.270865	-1.753134	2.201856	0.008629	0.704593
-46.081071	-1.788652	2.211853	0.008594	0.704590
-45.605707	-1.737021	2.221850	0.008505	0.704866
-45.232765	-1.792153	2.231846	0.008435	0.704889
-45.164923	-1.804920	2.241843	0.008422	0.704889
-45.512297	-1.743626	2.251840	0.008486	0.704888
-44.640518	-1.739196	2.261837	0.008323	0.705211
-44.695577	-1.730093	2.271834	0.008333	0.705210
-44.390849	-1.784974	2.281830	0.008276	0.705210
-44.360689	-1.721025	2.291827	0.008270	0.705350
-43.345164	-1.816566	2.301824	0.008081	0.705523
-43.629596	-1.767000	2.311821	0.008133	0.705522
-43.795466	-1.737134	2.321818	0.008164	0.705523
-42.964544	-1.770915	2.331814	0.008008	0.705754
-42.750605	-1.755331	2.341811	0.007968	0.705863
-42.585083	-1.786755	2.351808	0.007937	0.705860
-42.449702	-1.811328	2.361805	0.007911	0.705860
-42.165108	-1.745094	2.371802	0.007858	0.706096
-41.731374	-1.807537	2.381798	0.007777	0.706127
-41.918469	-1.774003	2.391795	0.007811	0.706128
-41.816379	-1.724687	2.401792	0.007792	0.706264
-41.077576	-1.769022	2.411789	0.007654	0.706441
-41.132630	-1.758793	2.421786	0.007664	0.706442
-40.846374	-1.800965	2.431782	0.007610	0.706461
-40.565852	-1.705652	2.441779	0.007557	0.706754
-40.225101	-1.767882	2.451776	0.007493	0.706751
-40.229315	-1.766755	2.461773	0.007494	0.706753
-39.903336	-1.700694	2.471770	0.007432	0.707003
-39.320225	-1.764981	2.481766	0.007324	0.707084
-39.417611	-1.747050	2.491763	0.007341	0.707086
-39.159484	-1.727668	2.501760	0.007293	0.707218
-38.577373	-1.753638	2.511757	0.007184	0.707375
-38.280681	-1.806884	2.521754	0.007128	0.707375
-38.343164	-1.794007	2.531750	0.007140	0.707379
-37.907022	-1.736983	2.541747	0.007058	0.707650
-37.580465	-1.771317	2.551744	0.006997	0.707699
-37.699769	-1.751155	2.561741	0.007018	0.707697
-37.387983	-1.740068	2.571738	0.006960	0.707832
-36.529098	-1.803872	2.581734	0.006800	0.708012
-36.872726	-1.741701	2.591731	0.006863	0.708014
-36.902866	-1.734275	2.601728	0.006868	0.708019
-35.998496	-1.732027	2.611725	0.006700	0.708348
-35.725502	-1.781280	2.621722	0.006648	0.708347
-35.688867	-1.786573	2.631718	0.006641	0.708351
-35.677457	-1.732804	2.641715	0.006639	0.708463
-34.748868	-1.811282	2.651712	0.006465	0.708638
-35.087064	-1.752734	2.661709	0.006528	0.708636
-34.976349	-1.773063	2.671706	0.006507	0.708635
-34.227232	-1.762779	2.681702	0.006367	0.708924
-34.092840	-1.769996	2.691699	0.006341	0.708958
-33.951134	-1.796590	2.701696	0.006315	0.708956
-34.070172	-1.725768	2.711693	0.006336	0.709057
-32.968701	-1.819587	2.721690	0.006131	0.709263
-33.111343	-1.794450	2.731686	0.006157	0.709263
-33.254148	-1.768346	2.741683	0.006183	0.709265
-32.557758	-1.755831	2.751680	0.006053	0.709539
-32.541058	-1.732250	2.761677	0.006049	0.709593
-32.186811	-1.796370	2.771674	0.005983	0.709592
-32.198899	-1.740459	2.781670	0.005985	0.709700
-31.327714	-1.797783	2.791667	0.005822	0.709897
-31.350139	-1.794970	2.801664	0.005826	0.709895
-31.324436	-1.801945	2.811661	0.005821	0.709891
-30.612481	-1.807205	2.821658	0.005688	0.710135
-30.647139	-1.758570	2.831654	0.005694	0.710221
-30.448879	-1.792074	2.841651	0.005657	0.710225
-30.613034	-1.729195	2.851648	0.005687	0.710293
-29.778149	-1.758126	2.861645	0.005531	0.710533
-29.459941	-1.815703	2.871642	0.005471	0.710532
-29.897936	-1.737621	2.881638	0.005552	0.710533
-28.996712	-1.763063	2.891635	0.005384	0.710804
-28.763453	-1.772073	2.901632	0.005340	0.710870
-28.781974	-1.769487	2.911629	0.005343	0.710869
-28.742950	-1.741648	2.921626	0.005336	0.710939
-27.978610	-1.776802	2.931622	0.005193	0.711142
-27.946770	-1.782564	2.941619	0.005187	0.711143
-28.203583	-1.738337	2.951616	0.005234	0.711140
-27.382997	-1.737451	2.961613	0.005081	0.711435
-27.197766	-1.761182	2.971610	0.005046	0.711454
-27.109388	-1.777567	2.981606	0.005029	0.711453
-26.827407	-1.743381	2.991603	0.004976	0.711623
-26.460238	-1.738739	3.001600	0.004907	0.711763
-26.388112	-1.751875	3.011597	0.004893	0.711763
-26.186368	-1.745380	3.021594	0.004855	0.711849
-25.340793	-1.773962	3.031590	0.004698	0.712093
-25.230014	-1.795004	3.041587	0.004676	0.712091
-25.464819	-1.752900	3.051584	0.004720	0.712092
-24.777534	-1.771277	3.061581	0.004591	0.712301
-24.482661	-1.782281	3.071578	0.004536	0.712384
-24.640649	-1.753355	3.081574	0.004565	0.712387
-24.349275	-1.775070	3.091571	0.004510	0.712448
-23.785355	-1.743226	3.101568	0.004405	0.712712
-23.537014	-1.789132	3.111565	0.004358	0.712709
-23.737499	-1.754754	3.121562	0.004395	0.712707
-23.063324	-1.761978	3.131558	0.004269	0.712933
-22.663656	-1.786822	3.141555	0.004194	0.713026
-22.828315	-1.758828	3.151552	0.004225	0.713024
-22.691814	-1.756767	3.161549	0.004199	0.713077
-22.163812	-1.709988	3.171546	0.004100	0.713359
-21.947492	-1.748302	3.181542	0.004059	0.713360
-21.848423	-1.765765	3.191539	0.004041	0.713361
-21.448219	-1.716162	3.201536	0.003966	0.713602
-21.235689	-1.729471	3.211533	0.003926	0.713652
-21.021560	-1.769870	3.221530	0.003885	0.713648
-20.765456	-1.754538	3.231526	0.003837	0.713770
-19.944751	-1.801013	3.241523	0.003684	0.713969
-20.233875	-1.750965	3.251520	0.003737	0.713967
-20.249275	-1.747640	3.261517	0.003740	0.713969
-19.557475	-1.729537	3.271514	0.003611	0.714251
-19.307428	-1.760166	3.281510	0.003564	0.714279
-19.311195	-1.759267	3.291507	0.003564	0.714280
-19.107353	-1.716188	3.301504	0.003525	0.714439
-18.202904	-1.792633	3.311501	0.003357	0.714608
-18.642923	-1.712989	3.321498	0.003438	0.714611
-18.280853	-1.778052	3.331494	0.003370	0.714611
-17.794825	-1.726459	3.341491	0.003279	0.714886
-17.728927	-1.726196	3.351488	0.003267	0.714910
-17.407164	-1.784235	3.361485	0.003206	0.714910
-17.572370	-1.673641	3.371482	0.003237	0.715072
-16.430459	-1.797701	3.381478	0.003024	0.715230
-16.653586	-1.757013	3.391475	0.003065	0.715233
-16.836682	-1.720660	3.401472	0.003098	0.715241
-15.975432	-1.722930	3.411469	0.002938	0.715541
-15.931089	-1.731546	3.421466	0.002929	0.715541
-15.647080	-1.780413	3.431462	0.002876	0.715545
-15.386498	-1.733452	3.441459	0.002827	0.715731
-14.741485	-1.770958	3.451456	0.002706	0.715885
-14.935219	-1.737518	3.461453	0.002742	0.715884
-14.879490	-1.748438	3.471450	0.002731	0.715883
-14.053067	-1.783055	3.481446	0.002577	0.716106
-13.886053	-1.799045	3.491443	0.002545	0.716135
-13.526737	-1.863651	3.501440	0.002478	0.716134
-13.504711	-1.868489	3.511437	0.002474	0.716133
-13.211907	-1.778919	3.521434	0.002419	0.716415
-12.657946	-1.859646	3.531430	0.002315	0.716451
-12.528817	-1.883247	3.541427	0.002291	0.716451
-12.443245	-1.899128	3.551424	0.002274	0.716450
-12.078287	-1.836321	3.561421	0.002206	0.716704
-11.730804	-1.872045	3.571418	0.002141	0.716757
-11.464136	-1.920500	3.581414	0.002091	0.716755
-11.677484	-1.882661	3.591411	0.002130	0.716756
-10.976387	-1.872955	3.601408	0.001999	0.717023
-10.992977	-1.839549	3.611405	0.002002	0.717084
-10.733965	-1.888259	3.621402	0.001953	0.717080
-10.444616	-1.940002	3.631398	0.001899	0.717080
-10.098758	-1.872090	3.641395	0.001834	0.717337
-9.926527	-1.882895	3.651392	0.001801	0.717377
-10.176414	-1.838035	3.661389	0.001848	0.717379
-9.873499	-1.842867	3.671386	0.001791	0.717477
-9.015898	-1.881332	3.681382	0.001631	0.717703
-9.051039	-1.873259	3.691379	0.001637	0.717708
-8.931694	-1.895432	3.701376	0.001614	0.717707
-8.670980	-1.825643	3.711373	0.001565	0.717937
-7.860094	-1.930204	3.721370	0.001414	0.718017
-7.896418	-1.924333	3.731366	0.001420	0.718016
-8.238942	-1.862500	3.741363	0.001483	0.718019
-7.304569	-1.860838	3.751360	0.001309	0.718352
-7.104785	-1.896070	3.761357	0.001271	0.718353
-6.821270	-1.946730	3.771354	0.001218	0.718353
-7.308096	-1.825157	3.781350	0.001308	0.718423
-6.202601	-1.909465	3.791347	0.001102	0.718646
-6.107123	-1.926317	3.801344	0.001084	0.718647
-6.439209	-1.868562	3.811341	0.001145	0.718645
-5.522129	-1.943037	3.821338	0.000974	0.718821
-5.343842	-1.905755	3.831334	0.000941	0.718958
-5.269815	-1.916726	3.841331	0.000926	0.718964
-5.228618	-1.926366	3.851328	0.000918	0.718960
-4.644690	-1.906987	3.861325	0.000809	0.719204
-4.306260	-1.935323	3.871322	0.000746	0.719268
-4.394999	-1.919247	3.881318	0.000762	0.719269
-4.330515	-1.913258	3.891315	0.000749	0.719304
-3.596922	-1.894221	3.901312	0.000612	0.719600
-3.376016	-1.933408	3.911309	0.000571	0.719601
-3.365542	-1.936983	3.921306	0.000569	0.719599
-3.400942	-1.859820	3.931302	0.000575	0.719739
-2.498028	-1.939749	3.941299	0.000406	0.719899
-2.712659	-1.902245	3.951296	0.000446	0.719899
-2.651391	-1.913279	3.961293	0.000434	0.719899
-2.098882	-1.848008	3.971290	0.000330	0.720222
-2.247438	-1.821239	3.981286	0.000358	0.720224
-1.938272	-1.874674	3.991283	0.000300	0.720228
-1.663530	-1.791342	4.001280	0.000248	0.720489
-1.475143	-1.800795	4.011277	0.000213	0.720537
-1.330476	-1.826482	4.021274	0.000185	0.720538
-1.245310	-1.695429	4.031270	0.000169	0.720827
-1.035091	-1.706175	4.041267	0.000129	0.720880
-1.000572	-1.685630	4.051264	0.000123	0.720933
-0.886294	-1.611779	4.061261	0.000101	0.721119
-0.920935	-1.604461	4.071258	0.000107	0.721122
-0.926943	-1.457808	4.081254	0.000107	0.721409
-0.820538	-1.462607	4.091251	0.000087	0.721438
-0.808567	-1.324101	4.101248	0.000084	0.721715
-0.862505	-1.281132	4.111245	0.000094	0.721782
-0.608720	-1.178017	4.121242	0.000046	0.722074
-0.778774	-1.085623	4.131238	0.000077	0.722196
-0.539118	-1.040058	4.141235	0.000032	0.722370
-0.367188	-0.929174	4.151232	-0.000000	0.722649
-0.364555	-0.854773	4.161229	-0.000001	0.722797
-0.432273	-0.736316	4.171226	0.000011	0.723006
-0.418878	-0.580498	4.181222	0.000008	0.723317
-0.262676	-0.508371	4.191219	-0.000022	0.723514
-0.205507	-0.407976	4.201216	-0.000033	0.723731
-0.303789	-0.263355	4.211213	-0.000015	0.723981
-0.120095	-0.152568	4.221210	-0.000050	0.724263
-0.048536	-0.012497	4.231206	-0.000063	0.724563
0.000000	0.120931	4.241203	-0.000073	0.724842

-0.038833	0.762552	4.246208	-0.000066	0.726083
-0.074459	2.036516	4.251213	-0.000061	0.728555
0.206729	3.858679	4.256218	-0.000114	0.732191
0.379423	6.240168	4.261222	-0.000148	0.736848
0.581854	9.133077	4.266227	-0.000188	0.742464
0.917146	12.486287	4.271232	-0.000253	0.748955
1.435045	16.254567	4.276237	-0.000352	0.756230
1.608768	20.496245	4.281242	-0.000387	0.764200
1.926706	25.106320	4.286246	-0.000450	0.772811
2.455467	30.051876	4.291251	-0.000552	0.782004
2.925892	35.350904	4.296256	-0.000643	0.791705
3.581791	40.935124	4.301261	-0.000769	0.801850
4.156932	46.853268	4.306266	-0.000880	0.812426
4.291131	53.112129	4.311270	-0.000909	0.823319
4.781204	59.597536	4.316275	-0.001005	0.834562
5.386774	66.264174	4.321280	-0.001122	0.845993
5.566853	73.236082	4.326285	-0.001161	0.857652
5.944590	80.382250	4.331290	-0.001236	0.869495
6.822910	87.617107	4.336294	-0.001404	0.881463
7.294856	95.115163	4.341299	-0.001497	0.893575
7.678739	102.774700	4.346304	-0.001574	0.905753
8.548575	110.502194	4.351309	-0.001741	0.918006
9.329733	118.367327	4.356314	-0.001892	0.930283
9.630271	126.405887	4.361318	-0.001953	0.942534
11.390101	134.320501	4.366323	-0.002286	0.954823
12.442070	142.448803	4.371328	-0.002488	0.967086
13.572191	150.661583	4.376333	-0.002704	0.979337
14.159081	159.078090	4.381338	-0.002819	0.991592
14.447109	167.556614	4.386342	-0.002878	1.003711
15.346502	175.982612	4.391347	-0.003051	1.015761
16.019978	184.481184	4.396352	-0.003182	1.027715
16.488529	193.052312	4.401357	-0.003276	1.039581
17.867764	201.500909	4.406362	-0.003538	1.051360
18.309811	210.136730	4.411366	-0.003626	1.063042
19.203515	218.734162	4.416371	-0.003798	1.074649
20.075162	227.326283	4.421376	-0.003967	1.086119
20.560640	236.005303	4.426381	-0.004063	1.097495
21.074964	244.683573	4.431386	-0.004164	1.108760
21.699024	253.329750	4.436390	-0.004286	1.119894
22.438752	261.967154	4.441395	-0.004430	1.130933
22.864098	270.643245	4.446400	-0.004515	1.141845
23.479433	279.308428	4.451405	-0.004636	1.152680
24.267188	287.908580	4.456410	-0.004788	1.163371
25.021352	296.493044	4.461414	-0.004934	1.173938
26.220852	305.013153	4.466419	-0.005163	1.184424
26.972594	313.609409	4.471424	-0.005309	1.194818
27.529383	322.214439	4.476429	-0.005419	1.205093
28.128039	330.819961	4.481434	-0.005536	1.215289
28.759964	339.378731	4.486438	-0.005659	1.225353
29.528990	347.951781	4.491443	-0.005808	1.235378
29.982428	356.506025	4.496448	-0.005899	1.245239
30.855199	364.999839	4.501453	-0.006067	1.255035
31.533234	373.514170	4.506458	-0.006199	1.264740
32.071043	382.046061	4.511462	-0.006305	1.274364
32.780268	390.525708	4.516467	-0.006443	1.283890
33.600070	398.996739	4.521472	-0.006601	1.293357
34.144638	407.479959	4.526477	-0.006708	1.302717
34.743288	416.046171	4.531482	-0.006825	1.312110
35.042122	424.563287	4.536486	-0.006887	1.321329
35.665805	432.967324	4.541491	-0.007009	1.330421
36.236974	441.374863	4.546496	-0.007121	1.339446
36.779149	449.768171	4.551501	-0.007227	1.348391
37.318649	458.181015	4.556506	-0.007333	1.357296
37.877593	466.535589	4.561510	-0.007443	1.366086
38.271201	474.951092	4.566515	-0.007522	1.374853
38.961288	483.293084	4.571520	-0.007656	1.383540
39.450307	491.681676	4.576525	-0.007753	1.392186
40.217478	499.995011	4.581530	-0.007901	1.400749
40.580157	508.358938	4.586534	-0.007975	1.409244
40.968731	516.738272	4.591539	-0.008053	1.417706
41.421058	525.062413	4.596544	-0.008143	1.426075
41.988554	533.386513	4.601549	-0.008254	1.434412
42.625379	541.679030	4.606554	-0.008378	1.442682
43.150349	549.975828	4.611558	-0.008481	1.450890
43.669760	558.291745	4.616563	-0.008584	1.459070
44.280004	566.577792	4.621568	-0.008703	1.467189
44.783671	574.931693	4.626573	-0.008802	1.475312
45.502188	583.178847	4.631578	-0.008942	1.483322
46.170899	591.425675	4.636582	-0.009072	1.491280
46.995350	599.670740	4.641587	-0.009231	1.499219
47.472743	607.954490	4.646592	-0.009325	1.507098
47.464288	616.320889	4.651597	-0.009330	1.514939
47.985876	624.569411	4.656602	-0.009432	1.522711
48.524097	632.809852	4.661606	-0.009538	1.530438
49.007697	641.075439	4.666611	-0.009634	1.538141
49.672598	649.285575	4.671616	-0.009763	1.545781
50.248845	657.541979	4.676621	-0.009876	1.553413
50.560151	665.806910	4.681626	-0.009940	1.560976
50.754156	674.069427	4.686630	-0.009981	1.568483
51.565653	682.258977	4.691635	-0.010138	1.575979
52.079533	690.475415	4.696640	-0.010239	1.583419
52.686056	698.683987	4.701645	-0.010358	1.590831
53.610558	706.861633	4.706650	-0.010535	1.598226
54.197208	715.047226	4.711654	-0.010650	1.605546
54.512357	723.338090	4.716659	-0.010714	1.612887
55.298418	731.498670	4.721664	-0.010866	1.620147
55.529076	739.763575	4.726669	-0.010915	1.627387
55.985335	748.045235	4.731674	-0.011005	1.634641
56.196920	756.253976	4.736678	-0.011050	1.641766
56.710302	764.438932	4.741683	-0.011151	1.648881
57.266759	772.622513	4.746688	-0.011261	1.655970
57.549432	780.828143	4.751693	-0.011319	1.663010
58.168820	788.999790	4.756698	-0.011440	1.670037
58.495887	797.212619	4.761702	-0.011506	1.677030
58.779833	805.409961	4.766707	-0.011565	1.683975
59.160825	813.605077	4.771712	-0.011641	1.690902
59.353098	821.818953	4.776717	-0.011682	1.697792
59.941113	829.964349	4.781722	-0.011797	1.704649
60.403340	838.146414	4.786726	-0.011889	1.711492
61.310990	846.257737	4.791731	-0.012064	1.718307
61.661837	854.416532	4.796736	-0.012134	1.725062
61.947690	862.607981	4.801741	-0.012193	1.731809
62.535919	870.765514	4.806746	-0.012308	1.738541
63.048319	878.897709	4.811750	-0.012409	1.745216
63.457801	887.097004	4.816755	-0.012491	1.751907
63.749853	895.287685	4.821760	-0.012551	1.758551
64.019228	903.432049	4.826765	-0.012607	1.765129
64.307100	911.626683	4.831770	-0.012666	1.771726
64.662433	919.787565	4.836774	-0.012737	1.778279
65.166213	927.909226	4.841779	-0.012837	1.784796
65.830770	936.063003	4.846784	-0.012966	1.791333
66.055895	944.263816	4.851789	-0.013013	1.797830
66.526508	952.381542	4.856794	-0.013107	1.804269
66.994175	960.495058	4.861798	-0.013199	1.810680
67.407497	968.656219	4.866803	-0.013282	1.817099
67.553680	976.830954	4.871808	-0.013314	1.823475
68.217791	984.923226	4.876813	-0.013444	1.829825
68.705183	993.074888	4.881818	-0.013540	1.836179
69.033374	1001.198454	4.886822	-0.013606	1.842470
69.540853	1009.327915	4.891827	-0.013706	1.848765
70.124734	1017.447692	4.896832	-0.013821	1.855040
70.518434	1025.593637	4.901837	-0.013899	1.861291
70.814261	1033.759250	4.906842	-0.013960	1.867525
71.059802	1041.939251	4.911846	-0.014011	1.873744
71.429404	1050.061634	4.916851	-0.014086	1.879912
71.644016	1058.202825	4.921856	-0.014131	1.886057
72.232646	1066.296186	4.926861	-0.014246	1.892188
72.647809	1074.436828	4.931866	-0.014329	1.898315
72.898275	1082.555000	4.936870	-0.014381	1.904387
73.226988	1090.705389	4.941875	-0.014448	1.910472
73.660584	1098.819083	4.946880	-0.014534	1.916522
74.121270	1106.898754	4.951885	-0.014625	1.922531
74.404503	1115.045361	4.956890	-0.014684	1.928551
74.892857	1123.148388	4.961894	-0.014780	1.934542
75.324081	1131.264176	4.966899	-0.014866	1.940518
76.091659	1139.338740	4.971904	-0.015014	1.946483
76.353656	1147.512250	4.976909	-0.015069	1.952445
76.915326	1155.613382	4.981914	-0.015179	1.958370
77.007714	1163.738501	4.986918	-0.015201	1.964243
77.250247	1171.874292	4.991923	-0.015252	1.970122
77.758683	1179.971386	4.996928	-0.015352	1.975985
78.062920	1188.075107	5.001933	-0.015414	1.981813
78.510185	1196.186928	5.006938	-0.015503	1.987644
78.688109	1204.336847	5.011942	-0.015542	1.993458
79.260906	1212.408432	5.016947	-0.015654	1.999240
79.699862	1220.483696	5.021952	-0.015741	2.004994
80.131245	1228.578339	5.026957	-0.015827	2.010744
80.532896	1236.704039	5.031962	-0.015907	2.016497
80.678920	1244.832380	5.036966	-0.015940	2.022208
81.030348	1252.926477	5.041971	-0.016011	2.027900
81.494668	1261.068048	5.046976	-0.016103	2.033622
81.595945	1269.187139	5.051981	-0.016127	2.039274
81.909191	1277.276740	5.056986	-0.016191	2.044912
82.084895	1285.381745	5.061990	-0.016229	2.050530
82.414949	1293.485620	5.066995	-0.016296	2.056149
82.958417	1301.546147	5.072000	-0.016403	2.061743
83.176635	1309.650770	5.077005	-0.016449	2.067320
83.573189	1317.778660	5.082010	-0.016528	2.072915
83.850962	1325.859022	5.087014	-0.016585	2.078451
84.156987	1333.959121	5.092019	-0.016648	2.083989
84.555802	1342.045178	5.097024	-0.016728	2.089511
84.791399	1350.162084	5.102029	-0.016777	2.095024
85.009500	1358.264638	5.107034	-0.016823	2.100510
85.428035	1366.326793	5.112038	-0.016907	2.105975
85.757574	1374.467586	5.117043	-0.016973	2.111469
86.269987	1382.559085	5.122048	-0.017074	2.116934
86.439426	1390.625573	5.127053	-0.017111	2.122335
86.852050	1398.692538	5.132058	-0.017194	2.127746
87.473514	1406.746110	5.137062	-0.017315	2.133154
87.771031	1414.849890	5.142067	-0.017376	2.138550
87.980984	1422.945067	5.147072	-0.017420	2.143919
88.908883	1430.944647	5.152077	-0.017598	2.149279
89.001514	1439.127358	5.157082	-0.017621	2.154668
89.306789	1447.189221	5.162086	-0.017684	2.159983
89.814278	1455.238772	5.167091	-0.017783	2.165297
90.120939	1463.353609	5.172096	-0.017846	2.170621
90.237616	1471.468569	5.177101	-0.017873	2.175914
90.574374	1479.552650	5.182106	-0.017941	2.181195
90.924113	1487.624108	5.187110	-0.018012	2.186456
91.163071	1495.755633	5.192115	-0.018062	2.191733
91.679567	1503.810493	5.197120	-0.018164	2.196973
92.197851	1511.845115	5.202125	-0.018266	2.202188
92.351140	1519.954294	5.207130	-0.018300	2.207405
92.551044	1528.053759	5.212134	-0.018342	2.212608
92.838558	1536.137369	5.217139	-0.018401	2.217796
93.152497	1544.206738	5.222144	-0.018465	2.222965
93.187409	1552.306720	5.227149	-0.018477	2.228117
93.594741	1560.399710	5.232154	-0.018559	2.233285
93.918104	1568.435561	5.237158	-0.018624	2.238398
94.237819	1576.510840	5.242163	-0.018689	2.243524
94.629178	1584.590373	5.247168	-0.018768	2.248647
94.884821	1592.685635	5.252173	-0.018821	2.253756
95.273584	1600.756275	5.257178	-0.018899	2.258850
95.838190	1608.789776	5.262182	-0.019009	2.263924
96.233421	1616.872709	5.267187	-0.019088	2.269003
96.926651	1625.008328	5.272192	-0.019223	2.274129
96.871823	1633.081103	5.277197	-0.019218	2.279140
97.183597	1641.138400	5.282202	-0.019282	2.284161
97.548203	1649.187428	5.287206	-0.019355	2.289171
97.633155	1657.309567	5.292211	-0.019376	2.294192
97.910878	1665.374096	5.297216	-0.019433	2.299182
98.228518	1673.404081	5.302221	-0.019498	2.304143
98.636783	1681.470273	5.307226	-0.019580	2.309124
98.860235	1689.569002	5.312230	-0.019627	2.314098
99.242882	1697.596505	5.317235	-0.019703	2.319031
99.323772	1705.696158	5.322240	-0.019724	2.323973
99.278314	1713.794354	5.327245	-0.019721	2.328892
99.574594	1721.880918	5.332250	-0.019782	2.333823
99.974252	1729.909572	5.337254	-0.019861	2.338716
100.310493	1737.963931	5.342259	-0.019929	2.343610
100.403158	1746.078999	5.347264	-0.019952	2.348510
100.823077	1754.140572	5.352269	-0.020036	2.353394
101.461712	1762.168811	5.357274	-0.020160	2.358265
101.380755	1770.253802	5.362278	-0.020151	2.363102
101.807403	1778.299733	5.367283	-0.020236	2.367947
102.171123	1786.382955	5.372288	-0.020309	2.372799
102.292791	1794.443324	5.377293	-0.020337	2.377609
102.663421	1802.509586	5.382298	-0.020411	2.382431
103.148720	1810.529399	5.387302	-0.020507	2.387226
103.520372	1818.625753	5.392307	-0.020582	2.392047
103.756913	1826.701185	5.397312	-0.020631	2.396835
103.915706	1834.759296	5.402317	-0.020666	2.401597
104.189698	1842.836505	5.407322	-0.020723	2.406370
104.446661	1850.894947	5.412326	-0.020776	2.411122
104.523065	1858.994770	5.417331	-0.020796	2.415874
104.946996	1867.021509	5.422336	-0.020880	2.420600
105.201310	1875.062049	5.427341	-0.020933	2.425313
105.360986	1883.191806	5.432346	-0.020968	2.430061
105.793764	1891.288094	5.437350	-0.021054	2.434801
105.966658	1899.312713	5.442355	-0.021092	2.439470
106.279686	1907.348418	5.447360	-0.021156	2.444148
106.785634	1915.363295	5.452365	-0.021255	2.448819
107.055040	1923.474684	5.457370	-0.021311	2.453519
107.066851	1931.544651	5.462374	-0.021319	2.458167
107.387456	1939.578911	5.467379	-0.021384	2.462808
107.705089	1947.642824	5.472384	-0.021448	2.467457
107.838472	1955.720537	5.477389	-0.021479	2.472092
108.094157	1963.792657	5.482394	-0.021532	2.476724
108.498680	1971.817974	5.487398	-0.021613	2.481332
108.671387	1979.862227	5.492403	-0.021650	2.485924
108.852513	1987.963552	5.497408	-0.021689	2.490542
109.026576	1996.020624	5.502413	-0.021727	2.495124
109.599862	2004.055656	5.507418	-0.021839	2.499716
109.748052	2012.102080	5.512422	-0.021873	2.504274
110.199551	2020.138032	5.517427	-0.021962	2.508840
110.550348	2028.251544	5.522432	-0.022033	2.513434
110.829101	2036.278466	5.527437	-0.022090	2.517965
111.097899	2044.316295	5.532442	-0.022146	2.522494
111.390616	2052.354245	5.537446	-0.022206	2.527016
111.812269	2060.395887	5.542451	-0.022290	2.531542
112.224735	2068.472124	5.547456	-0.022372	2.536078
112.390576	2076.520757	5.552461	-0.022408	2.540573
112.709844	2084.577713	5.557466	-0.022473	2.545075
112.979089	2092.641427	5.562470	-0.022529	2.549570
113.287783	2100.721873	5.567475	-0.022592	2.554068
113.515295	2108.770269	5.572480	-0.022640	2.558536
113.780790	2116.786194	5.577485	-0.022694	2.562980
114.064806	2124.866309	5.582490	-0.022753	2.567453
114.167113	2132.945563	5.587494	-0.022777	2.571905
114.680608	2140.974878	5.592499	-0.022878	2.576350
114.903279	2149.040415	5.597504	-0.022925	2.580788
115.250697	2157.063785	5.602509	-0.022995	2.585203
115.669298	2165.131344	5.607514	-0.023079	2.589640
115.728503	2173.406929	5.612518	-0.023095	2.594158
115.797441	2181.405390	5.617523	-0.023114	2.598518
116.052685	2189.427433	5.622528	-0.023167	2.602896
116.120148	2197.420606	5.627533	-0.023185	2.607238
116.547169	2205.440401	5.632538	-0.023270	2.611611
116.641888	2213.505924	5.637542	-0.023293	2.615980
116.923114	2221.510948	5.642547	-0.023350	2.620321
117.201431	2229.539058	5.647552	-0.023408	2.624667
117.508255	2237.580902	5.652557	-0.023470	2.629015
117.669688	2245.676291	5.657562	-0.023506	2.633375
118.090467	2253.683056	5.662566	-0.023590	2.637698
118.291014	2261.722132	5.667571	-0.023632	2.642016
118.735901	2269.753542	5.672576	-0.023721	2.646339
119.224616	2277.781860	5.677581	-0.023817	2.650656
119.451064	2285.883522	5.682586	-0.023865	2.654988
119.659423	2293.913843	5.687590	-0.023909	2.659273
119.978860	2301.956050	5.692595	-0.023974	2.663565
120.263777	2310.033310	5.697600	-0.024033	2.667867
120.398558	2318.108401	5.702605	-0.024063	2.672150
120.605584	2326.186584	5.707610	-0.024107	2.676434
120.914000	2334.200415	5.712614	-0.024170	2.680682
121.225155	2342.202502	5.717619	-0.024233	2.684918
121.556234	2350.260745	5.722624	-0.024300	2.689178
121.839211	2358.315759	5.727629	-0.024359	2.693427
122.074283	2366.378710	5.732634	-0.024408	2.697669
122.187161	2374.413095	5.737638	-0.024434	2.701883
122.543525	2382.436840	5.742643	-0.024506	2.706099
122.939848	2390.499655	5.747648	-0.024585	2.710332
123.104283	2398.556894	5.752653	-0.024621	2.714541
123.528966	2406.589642	5.757658	-0.024706	2.718747
123.844640	2414.618011	5.762662	-0.024770	2.722937
124.046125	2422.658680	5.767667	-0.024813	2.727120
124.121277	2430.757004	5.772672	-0.024833	2.731318
124.439157	2438.791294	5.777677	-0.024897	2.735492
124.769940	2446.821991	5.782682	-0.024964	2.739658
124.934941	2454.867147	5.787686	-0.025000	2.743815
125.084704	2462.924586	5.792691	-0.025034	2.747972
125.264303	2471.043084	5.797696	-0.025073	2.752155
125.424772	2479.106885	5.802701	-0.025108	2.756302
125.793926	2487.106574	5.807706	-0.025182	2.760424
125.987343	2495.094472	5.812710	-0.025224	2.764522
126.185008	2503.152559	5.817715	-0.025266	2.768650
126.450193	2511.216122	5.822720	-0.025321	2.772779
126.619870	2519.257618	5.827725	-0.025358	2.776885
126.889859	2527.292055	5.832730	-0.025414	2.780987
127.224587	2535.292222	5.837734	-0.025481	2.785069
127.538970	2543.333797	5.842739	-0.025545	2.789165
127.770069	2551.427891	5.847744	-0.025594	2.793277
127.705133	2559.463881	5.852749	-0.025587	2.797336
128.162834	2567.479580	5.857754	-0.025678	2.801409
128.374997	2575.508269	5.862758	-0.025723	2.805468
128.569582	2583.559428	5.867763	-0.025764	2.809532
128.819609	2591.634634	5.872768	-0.025816	2.813606
129.063065	2599.667664	5.877773	-0.025867	2.817651
129.355147	2607.699954	5.882778	-0.025927	2.821694
129.397514	2615.748779	5.887782	-0.025940	2.825724
129.817553	2623.753489	5.892787	-0.026024	2.829749
130.096417	2631.861061	5.897792	-0.026081	2.833810
130.013595	2639.913755	5.902797	-0.026072	2.837818
130.214030	2647.947494	5.907802	-0.026114	2.841827
130.523068	2655.944539	5.912806	-0.026177	2.845818
130.472501	2664.003153	5.917811	-0.026173	2.849814
130.918584	2672.044660	5.922816	-0.026262	2.853824
131.212961	2680.057390	5.927821	-0.026322	2.857805
131.543145	2688.090708	5.932826	-0.026389	2.861793
131.588061	2696.159901	5.937830	-0.026403	2.865777
131.895514	2704.186789	5.942835	-0.026465	2.869749
132.343529	2712.271448	5.947840	-0.026554	2.873752
132.393582	2720.279899	5.952845	-0.026569	2.877689
132.657677	2728.310470	5.957850	-0.026624	2.881644
132.851467	2736.371539	5.962854	-0.026665	2.885605
132.984970	2744.381552	5.967859	-0.026696	2.889532
133.188255	2752.484296	5.972864	-0.026739	2.893502
133.401089	2760.493516	5.977869	-0.026784	2.897422
133.760772	2768.526939	5.982874	-0.026856	2.901357
133.812005	2776.587579	5.987878	-0.026871	2.905282
134.167942	2784.598547	5.992883	-0.026943	2.909195
134.512322	2792.737638	5.997888	-0.027013	2.913163
134.546737	2800.749347	6.002893	-0.027025	2.917048
134.824262	2808.763807	6.007898	-0.027082	2.920943
135.198983	2816.726123	6.012902	-0.027157	2.924811
135.393647	2824.769353	6.017907	-0.027199	2.928704
135.628751	2832.834537	6.022912	-0.027248	2.932605
135.669460	2840.881807	6.027917	-0.027261	2.936482
135.899435	2848.900316	6.032922	-0.027309	2.940349
136.060530	2856.916170	6.037926	-0.027345	2.944207
136.290588	2864.963172	6.042931	-0.027393	2.948078
136.689599	2873.021523	6.047936	-0.027473	2.951958
136.711095	2881.079202	6.052941	-0.027482	2.955813
137.118100	2889.080366	6.057946	-0.027563	2.959656
137.496048	2897.074978	6.062950	-0.027639	2.963489
137.624792	2905.116088	6.067955	-0.027668	2.967326
137.851838	2913.207705	6.072960	-0.027716	2.971188
138.007757	2921.246583	6.077965	-0.027751	2.975016
138.138900	2929.287361	6.082970	-0.027781	2.978839
138.249654	2937.322261	6.087974	-0.027807	2.982652
138.414554	2945.343931	6.092979	-0.027843	2.986458
138.891254	2953.391711	6.097984	-0.027937	2.990286
139.130389	2961.461355	6.102989	-0.027987	2.994108
139.267129	2969.486026	6.107994	-0.028018	2.997899
139.404677	2977.504265	6.112998	-0.028049	3.001682
139.625143	2985.518642	6.118003	-0.028095	3.005462
139.749279	2993.547386	6.123008	-0.028124	3.009240
139.807497	3001.618518	6.128013	-0.028140	3.013029
140.007275	3009.660339	6.133018	-0.028183	3.016807
140.215666	3017.692760	6.138022	-0.028227	3.020577
140.338676	3025.695456	6.143027	-0.028256	3.024323
140.736042	3033.729733	6.148032	-0.028335	3.028093
140.836623	3041.797082	6.153037	-0.028359	3.031859
140.992329	3049.859404	6.158042	-0.028394	3.035621
141.471888	3057.808898	6.163046	-0.028488	3.039341
141.727139	3065.847421	6.168051	-0.028541	3.043087
142.053337	3073.889336	6.173056	-0.028607	3.046833
142.252309	3081.922078	6.178061	-0.028650	3.050565
142.532075	3089.996282	6.183066	-0.028708	3.054315
142.812743	3098.022341	6.188070	-0.028765	3.058038
142.593260	3106.081859	6.193075	-0.028730	3.061748
143.077720	3114.097995	6.198080	-0.028825	3.065467
143.445927	3122.106146	6.203085	-0.028899	3.069172
143.582250	3130.246288	6.208090	-0.028930	3.072922
143.579018	3138.291647	6.213094	-0.028935	3.076618
143.633872	3146.272025	6.218099	-0.028951	3.080282
143.805978	3154.274597	6.223104	-0.028988	3.083958
143.966358	3162.292776	6.228109	-0.029024	3.087636
144.226995	3170.349429	6.233114	-0.029078	3.091331
144.293749	3178.410771	6.238118	-0.029095	3.095015
144.281028	3186.434961	6.243123	-0.029099	3.098675
144.751651	3194.441382	6.248128	-0.029192	3.102344
145.036559	3202.442491	6.253133	-0.029250	3.105997
145.165648	3210.493497	6.258138	-0.029280	3.109662
145.315989	3218.569158	6.263142	-0.029313	3.113335
145.746599	3226.559008	6.268147	-0.029399	3.116977
145.853758	3234.618169	6.273152	-0.029424	3.120632
145.934299	3242.610061	6.278157	-0.029444	3.124251
146.311363	3250.639988	6.283162	-0.029520	3.127895
146.342410	3258.715746	6.288166	-0.029531	3.131541
146.350913	3266.750492	6.293171	-0.029538	3.135163
146.882993	3274.724279	6.298176	-0.029643	3.138777
147.138503	3282.756230	6.303181	-0.029696	3.142401
147.186534	3290.818622	6.308186	-0.029710	3.146024
147.319517	3298.868802	6.313190	-0.029741	3.149642
147.720965	3306.911858	6.318195	-0.029821	3.153264
147.985336	3314.960982	6.323200	-0.029875	3.156879
147.970649	3322.955785	6.328205	-0.029878	3.160453
148.231139	3330.972099	6.333210	-0.029932	3.164044
148.486766	3338.993229	6.338214	-0.029985	3.167634
148.565649	3347.054698	6.343219	-0.030005	3.171229
148.793811	3355.108155	6.348224	-0.030053	3.174824
148.914195	3363.131351	6.353229	-0.030081	3.178396
149.206759	3371.134435	6.358234	-0.030141	3.181963
149.355167	3379.171037	6.363238	-0.030174	3.185534
149.824770	3387.173313	6.368243	-0.030267	3.189099
149.759139	3395.288129	6.373248	-0.030260	3.192688
149.948890	3403.309280	6.378253	-0.030301	3.196242
150.300198	3411.291556	6.383258	-0.030372	3.199782
150.369094	3419.350730	6.388262	-0.030390	3.203340
150.433612	3427.373238	6.393267	-0.030407	3.206877
150.838886	3435.405083	6.398272	-0.030488	3.210429
151.054393	3443.429115	6.403277	-0.030534	3.213966
151.180640	3451.476192	6.408282	-0.030563	3.217505
151.104973	3459.535500	6.413286	-0.030554	3.221037
151.245657	3467.499937	6.418291	-0.030586	3.224533
151.666144	3475.552539	6.423296	-0.030670	3.228075
151.811769	3483.598421	6.428301	-0.030702	3.231599
151.955787	3491.676918	6.433306	-0.030734	3.235133
152.460266	3499.624846	6.438310	-0.030834	3.238621
152.487856	3507.673862	6.443315	-0.030844	3.242130
152.559568	3515.714619	6.448320	-0.030863	3.245633
152.851118	3523.689202	6.453325	-0.030923	3.249112
153.047808	3531.748825	6.458330	-0.030965	3.252621
153.319921	3539.808878	6.463334	-0.031021	3.256129
153.250233	3547.810406	6.468339	-0.031014	3.259595
153.273372	3555.877572	6.473344	-0.031023	3.263088
153.401957	3563.881653	6.478349	-0.031053	3.266555
153.573007	3571.912847	6.483354	-0.031090	3.270032
154.020360	3579.950691	6.488358	-0.031179	3.273519
154.318079	3587.966724	6.493363	-0.031240	3.276986
154.666918	3596.003449	6.498368	-0.031310	3.280461
155.009742	3603.969547	6.503373	-0.031379	3.283902
155.312038	3612.017607	6.508378	-0.031441	3.287372
155.796437	3620.077576	6.513382	-0.031537	3.290851
155.880253	3628.125491	6.518387	-0.031558	3.294305
156.239381	3636.152846	6.523392	-0.031630	3.297758
156.302751	3644.162696	6.528397	-0.031647	3.301188
156.474315	3652.170527	6.533402	-0.031685	3.304618
156.581215	3660.240072	6.538406	-0.031710	3.308068
156.847125	3668.283467	6.543411	-0.031765	3.311509
157.088414	3676.347810	6.548416	-0.031815	3.314955
157.159712	3684.338119	6.553421	-0.031834	3.318359
157.387918	3692.349264	6.558426	-0.031882	3.321775
157.350156	3700.372349	6.563430	-0.031880	3.325182
157.370612	3708.397799	6.568435	-0.031890	3.328589
157.949383	3716.425992	6.573440	-0.032003	3.332014
158.040281	3724.471497	6.578445	-0.032025	3.335425
158.001724	3732.519611	6.583450	-0.032024	3.338828
158.360666	3740.517647	6.588454	-0.032096	3.342222
158.528594	3748.505083	6.593459	-0.032132	3.345601
158.742567	3756.578150	6.598464	-0.032178	3.349013
158.970283	3764.605739	6.603469	-0.032226	3.352404
159.207866	3772.651109	6.608474	-0.032275	3.355799
159.250651	3780.651703	6.613478	-0.032289	3.359165
159.265606	3788.669433	6.618483	-0.032297	3.362534
159.790270	3796.696166	6.623488	-0.032400	3.365921
159.782596	3804.711969	6.628493	-0.032404	3.369282
160.030452	3812.778850	6.633498	-0.032456	3.372669
160.196566	3820.835546	6.638502	-0.032492	3.376046
160.445121	3828.803709	6.643507	-0.032544	3.379385
160.523421	3836.866876	6.648512	-0.032564	3.382755
160.618887	3844.890998	6.653517	-0.032587	3.386105
161.068474	3852.908226	6.658522	-0.032676	3.389462
161.465417	3860.995829	6.663526	-0.032756	3.392843
161.646346	3869.015207	6.668531	-0.032795	3.396184
162.096799	3877.032016	6.673536	-0.032884	3.399531
162.312553	3884.970459	6.678541	-0.032930	3.402833
162.579573	3893.022426	6.683546	-0.032985	3.406181
162.799043	3901.044179	6.688550	-0.033031	3.409512
162.758293	3909.086435	6.693555	-0.033029	3.412838
162.933946	3917.153356	6.698560	-0.033067	3.416180
162.900141	3925.127597	6.703565	-0.033066	3.419472
163.273750	3933.138000	6.708570	-0.033141	3.422790
163.565845	3941.200191	6.713574	-0.033201	3.426124
163.638699	3949.214039	6.718579	-0.033220	3.429426
164.070377	3957.265499	6.723584	-0.033306	3.432753
164.339999	3965.285019	6.728589	-0.033361	3.436059
164.465222	3973.261782	6.733594	-0.033390	3.439338
164.705606	3981.311484	6.738598	-0.033440	3.442649
165.061887	3989.317738	6.743603	-0.033512	3.445942
165.290728	3997.368071	6.748608	-0.033560	3.449245
165.373921	4005.425771	6.753613	-0.033581	3.452544
165.689720	4013.463329	6.758618	-0.033645	3.455839
165.822867	4021.488950	6.763622	-0.033676	3.459120
165.970615	4029.489693	6.768627	-0.033709	3.462388
166.262864	4037.537882	6.773632	-0.033768	3.465677
166.272374	4045.554249	6.778637	-0.033776	3.468941
166.296282	4053.626185	6.783642	-0.033786	3.472225
166.556742	4061.692397	6.788646	-0.033840	3.475510
166.619421	4069.652755	6.793651	-0.033857	3.478744
166.950202	4077.654074	6.798656	-0.033924	3.482000
166.868953	4085.657713	6.803661	-0.033914	3.485240
167.027755	4093.700069	6.808666	-0.033949	3.488501
167.344435	4101.751562	6.813670	-0.034013	3.491767
167.263621	4109.762190	6.818675	-0.034004	3.495001
167.512891	4117.799353	6.823680	-0.034056	3.498253
167.791132	4125.785327	6.828685	-0.034113	3.501482
167.837887	4133.796766	6.833690	-0.034127	3.504712
168.077294	4141.844944	6.838694	-0.034177	3.507959
168.411299	4149.856892	6.843699	-0.034245	3.511192
168.682597	4157.899094	6.848704	-0.034301	3.514431
168.827462	4165.941440	6.853709	-0.034333	3.517664
169.191545	4173.933967	6.858714	-0.034406	3.520881
169.267552	4181.926367	6.863718	-0.034426	3.524085
169.588364	4189.965165	6.868723	-0.034491	3.527313
169.766833	4198.043389	6.873728	-0.034530	3.530550
169.907958	4206.076447	6.878733	-0.034561	3.533764
169.920922	4214.116411	6.883738	-0.034569	3.536974
170.287624	4222.120564	6.888742	-0.034643	3.540177
170.463148	4230.126930	6.893747	-0.034681	3.543373
170.979638	4238.157391	6.898752	-0.034783	3.546585
171.012828	4246.204851	6.903757	-0.034794	3.549787
171.176475	4254.315098	6.908762	-0.034830	3.553015
171.668433	4262.348570	6.913766	-0.034927	3.556219
171.578730	4270.301216	6.918771	-0.034916	3.559371
172.112668	4278.279313	6.923776	-0.035021	3.562549
172.165236	4286.306652	6.928781	-0.035036	3.565729
172.296861	4294.332996	6.933786	-0.035066	3.568908
172.449167	4302.397444	6.938790	-0.035100	3.572100
172.862182	4310.384427	6.943795	-0.035182	3.575266
172.962124	4318.413443	6.948800	-0.035206	3.578437
173.036341	4326.438039	6.953805	-0.035226	3.581602
173.363265	4334.410956	6.958810	-0.035292	3.584752
173.537075	4342.469612	6.963814	-0.035330	3.587928
173.814434	4350.497817	6.968819	-0.035387	3.591092
173.861755	4358.534718	6.973824	-0.035401	3.594250
174.183144	4366.551046	6.978829	-0.035466	3.597405
174.116473	4374.562571	6.983834	-0.035459	3.600545
174.382076	4382.558892	6.988838	-0.035514	3.603685
174.369756	4390.614858	6.993843	-0.035517	3.606838
174.816832	4398.615640	6.998848	-0.035606	3.609979
175.062444	4406.665074	7.003853	-0.035657	3.613131
175.415353	4414.714063	7.008858	-0.035728	3.616283
175.822463	4422.666321	7.013862	-0.035810	3.619396
176.014736	4430.685614	7.018867	-0.035851	3.622526
176.223753	4438.730016	7.023872	-0.035895	3.625664
176.406949	4446.764026	7.028877	-0.035935	3.628795
176.697952	4454.831291	7.033882	-0.035994	3.631938
176.644402	4462.896684	7.038886	-0.035990	3.635069
176.784735	4470.886335	7.043891	-0.036021	3.638173
177.196858	4478.914828	7.048896	-0.036104	3.641296
177.198814	4486.885173	7.053901	-0.036109	3.644384
177.435333	4494.946217	7.058906	-0.036159	3.647510
177.795718	4502.977522	7.063910	-0.036231	3.650625
177.949307	4511.000901	7.068915	-0.036265	3.653729
178.010461	4519.071467	7.073920	-0.036282	3.656846
178.279658	4527.032766	7.078925	-0.036338	3.659923
178.730511	4534.995056	7.083930	-0.036427	3.663004
179.035929	4543.079548	7.088934	-0.036490	3.666124
179.111609	4551.105377	7.093939	-0.036509	3.669214
179.349044	4559.166952	7.098944	-0.036559	3.672319
179.686147	4567.188117	7.103949	-0.036627	3.675408
179.973073	4575.166636	7.108954	-0.036686	3.678477
180.248717	4583.209730	7.113958	-0.036743	3.681568
180.366218	4591.184615	7.118963	-0.036770	3.684626
180.513179	4599.249097	7.123968	-0.036803	3.687716
180.785527	4607.264764	7.128973	-0.036859	3.690789
181.005582	4615.284145	7.133978	-0.036905	3.693858
181.310799	4623.313707	7.138982	-0.036967	3.696932
181.318447	4631.300806	7.143987	-0.036974	3.699979
181.370323	4639.361264	7.148992	-0.036989	3.703052
181.628677	4647.366621	7.153997	-0.037043	3.706108
181.881361	4655.386461	7.159002	-0.037095	3.709166
182.561984	4663.488034	7.164006	-0.037228	3.712263
182.614696	4671.537708	7.169011	-0.037243	3.715322
182.957959	4679.490607	7.174016	-0.037312	3.718349
183.158114	4687.484851	7.179021	-0.037355	3.721386
183.449759	4695.451024	7.184026	-0.037415	3.724412
183.564109	4703.517599	7.189030	-0.037441	3.727469
183.662517	4711.543160	7.194035	-0.037465	3.730507
183.726448	4719.613854	7.199040	-0.037483	3.733560
183.908850	4727.605151	7.204045	-0.037522	3.736582
184.127872	4735.586631	7.209050	-0.037568	3.739600
184.269684	4743.644112	7.214054	-0.037600	3.742642
184.622035	4751.627901	7.219059	-0.037671	3.745658
184.893420	4759.671456	7.224064	-0.037727	3.748693
185.116610	4767.719671	7.229069	-0.037774	3.751725
185.702602	4775.747032	7.234074	-0.037889	3.754756
185.933449	4783.744872	7.239078	-0.037937	3.757765
185.983124	4791.782862	7.244083	-0.037952	3.760783
186.330226	4799.799081	7.249088	-0.038022	3.763796
186.419030	4807.847696	7.254093	-0.038044	3.766814
186.611184	4815.852287	7.259098	-0.038085	3.769815
186.826077	4823.917075	7.264102	-0.038130	3.772836
186.986921	4831.922346	7.269107	-0.038166	3.775832
187.231604	4839.926477	7.274112	-0.038217	3.778826
187.482776	4847.944214	7.279117	-0.038269	3.781824
187.730835	4855.956889	7.284122	-0.038321	3.784817
188.125993	4863.985664	7.289126	-0.038400	3.787817
187.956480	4872.031170	7.294131	-0.038374	3.790808
188.315984	4880.104416	7.299136	-0.038446	3.793819
188.361125	4888.120513	7.304141	-0.038460	3.796799
188.524987	4896.045935	7.309146	-0.038496	3.799746
188.935967	4904.064042	7.314150	-0.038578	3.802730
189.113811	4912.070303	7.319155	-0.038616	3.805703
189.376207	4920.118429	7.324160	-0.038670	3.808690
189.536982	4928.162045	7.329165	-0.038706	3.811671
189.808911	4936.170118	7.334170	-0.038762	3.814639
189.919318	4944.229393	7.339174	-0.038788	3.817620
190.040849	4952.205588	7.344179	-0.038816	3.820569
190.242544	4960.219787	7.349184	-0.038859	3.823531
190.596859	4968.237478	7.354189	-0.038930	3.826495
190.414140	4976.276111	7.359194	-0.038902	3.829453
190.795323	4984.345630	7.364198	-0.038978	3.832432
190.885346	4992.337939	7.369203	-0.039000	3.835374
190.884434	5000.349217	7.374208	-0.039006	3.838319
191.016332	5008.357474	7.379213	-0.039036	3.841263
191.266300	5016.337231	7.384218	-0.039088	3.844197
191.600850	5024.399368	7.389222	-0.039155	3.847161
191.719842	5032.404895	7.394227	-0.039183	3.850097
192.030157	5040.437521	7.399232	-0.039246	3.853045
192.146188	5048.480366	7.404237	-0.039273	3.855991
192.265961	5056.509565	7.409242	-0.039301	3.858929
192.565474	5064.522241	7.414246	-0.039362	3.861862
192.893593	5072.494236	7.419251	-0.039429	3.864779
192.996924	5080.580562	7.424256	-0.039453	3.867731
193.152900	5088.587999	7.429261	-0.039488	3.870653
193.312274	5096.852622	7.434266	-0.039523	3.873666
193.588539	5104.845412	7.439270	-0.039580	3.876580
193.670735	5112.708787	7.444275	-0.039601	3.879442
193.659740	5120.737703	7.449280	-0.039604	3.882359
193.793069	5128.745171	7.454285	-0.039634	3.885270
193.970683	5136.704707	7.459290	-0.039673	3.888161
194.123585	5144.755977	7.464294	-0.039707	3.891083
194.261427	5152.795204	7.469299	-0.039738	3.893999
194.456762	5160.792638	7.474304	-0.039780	3.896898
194.684135	5168.768538	7.479309	-0.039827	3.899788
194.987089	5176.789709	7.484314	-0.039889	3.902693
195.293331	5184.844492	7.489318	-0.039952	3.905608
195.307112	5192.838396	7.494323	-0.039960	3.908494
195.660968	5200.938418	7.499328	-0.040031	3.911422
195.967173	5208.921470	7.504333	-0.040093	3.914305
195.969316	5216.935673	7.509338	-0.040099	3.917191
196.250662	5224.899011	7.514342	-0.040157	3.920062
196.503291	5232.915805	7.519347	-0.040210	3.922950
196.690989	5240.958426	7.524352	-0.040250	3.925843
196.671754	5248.991423	7.529357	-0.040252	3.928727
196.948937	5257.010191	7.534362	-0.040309	3.931609
197.394716	5265.041333	7.539366	-0.040397	3.934497
197.234814	5273.065210	7.544371	-0.040373	3.937369
197.597771	5281.080237	7.549376	-0.040446	3.940245
197.800757	5289.069917	7.554381	-0.040489	3.943107
198.047369	5297.095669	7.559386	-0.040541	3.945980
198.331635	5305.149139	7.564390	-0.040599	3.948862
198.199651	5313.172118	7.569395	-0.040580	3.951724
198.517073	5321.228870	7.574400	-0.040644	3.954603
198.608229	5329.234276	7.579405	-0.040667	3.957458
198.869860	5337.209210	7.584410	-0.040721	3.960304
199.057083	5345.233942	7.589414	-0.040761	3.963163
199.285479	5353.187066	7.594419	-0.040809	3.965996
199.448602	5361.215002	7.599424	-0.040845	3.968852
199.906330	5369.290186	7.604429	-0.040936	3.971727
200.248691	5377.295049	7.609434	-0.041005	3.974574
200.388851	5385.341760	7.614438	-0.041036	3.977430
200.488685	5393.326595	7.619443	-0.041060	3.980261
200.875104	5401.367256	7.624448	-0.041138	3.983115
200.737808	5409.392361	7.629453	-0.041118	3.985953
200.850760	5417.420357	7.634458	-0.041144	3.988793
200.962790	5425.457708	7.639462	-0.041170	3.991635
201.082056	5433.493434	7.644467	-0.041198	3.994475
201.373204	5441.500510	7.649472	-0.041258	3.997305
201.727183	5449.483067	7.654477	-0.041329	4.000125
201.896860	5457.509922	7.659482	-0.041366	4.002956
201.947343	5465.563895	7.664486	-0.041381	4.005793
202.215516	5473.556108	7.669491	-0.041436	4.008609
202.489888	5481.625732	7.674496	-0.041493	4.011451
202.550012	5489.657434	7.679501	-0.041509	4.014274
202.703756	5497.685324	7.684506	-0.041544	4.017095
202.961827	5505.674257	7.689510	-0.041597	4.019902
203.028863	5513.677306	7.694515	-0.041615	4.022709
203.337862	5521.696761	7.699520	-0.041678	4.025523
203.442556	5529.726427	7.704525	-0.041703	4.028336
203.881811	5537.746321	7.709530	-0.041790	4.031149
204.008950	5545.920403	7.714534	-0.041819	4.034009
204.209806	5553.886205	7.719539	-0.041862	4.036795
204.380770	5561.822209	7.724544	-0.041899	4.039568
204.468733	5569.819207	7.729549	-0.041921	4.042359
204.531159	5577.799572	7.734554	-0.041938	4.045143
205.034358	5585.828672	7.739558	-0.042037	4.047948
205.229007	5593.838877	7.744563	-0.042079	4.050739
205.223559	5601.899888	7.749568	-0.042083	4.053544
205.565690	5609.891802	7.754573	-0.042153	4.056327
205.415281	5617.872055	7.759578	-0.042130	4.059098
205.727284	5625.924047	7.764582	-0.042193	4.061898
206.014571	5633.889136	7.769587	-0.042252	4.064666
206.215232	5641.947999	7.774592	-0.042295	4.067463
206.203326	5649.990515	7.779597	-0.042298	4.070249
206.493911	5658.016356	7.784602	-0.042358	4.073032
206.754488	5666.052638	7.789606	-0.042412	4.075816
206.730562	5674.011116	7.794611	-0.042413	4.078567
206.768419	5682.057459	7.799616	-0.042425	4.081348
206.993525	5690.018654	7.804621	-0.042473	4.084100
207.226368	5698.074618	7.809626	-0.042522	4.086883
207.528576	5706.088161	7.814630	-0.042583	4.089651
207.531557	5714.136211	7.819635	-0.042589	4.092424
208.035195	5722.152069	7.824640	-0.042688	4.095191
208.213313	5730.199809	7.829645	-0.042727	4.097963
208.173685	5738.183380	7.834650	-0.042725	4.100707
208.372261	5746.209492	7.839654	-0.042768	4.103468
208.631591	5754.197853	7.844659	-0.042821	4.106215
208.696690	5762.252755	7.849664	-0.042839	4.108980
208.893514	5770.315421	7.854669	-0.042881	4.111748
209.036840	5778.318188	7.859674	-0.042913	4.114492
209.412543	5786.374204	7.864678	-0.042988	4.117256
209.459311	5794.284710	7.869683	-0.043003	4.119964
209.751923	5802.330131	7.874688	-0.043062	4.122720
210.067080	5810.319013	7.879693	-0.043127	4.125454
209.899142	5818.382244	7.884698	-0.043101	4.128206
210.113922	5826.464288	7.889702	-0.043146	4.130968
210.324043	5834.432985	7.894707	-0.043191	4.133689
210.506969	5842.528940	7.899712	-0.043230	4.136451
210.651065	5850.491517	7.904717	-0.043263	4.139165
210.918260	5858.493525	7.909722	-0.043318	4.141892
211.222373	5866.441782	7.914726	-0.043380	4.144600
211.184979	5874.513060	7.919731	-0.043378	4.147344
211.487659	5882.563952	7.924736	-0.043440	4.150083
211.756536	5890.579163	7.929741	-0.043496	4.152807
211.765588	5898.614297	7.934746	-0.043503	4.155534
212.059739	5906.594224	7.939750	-0.043563	4.158243
212.170472	5914.642920	7.944755	-0.043589	4.160971
212.409880	5922.627082	7.949760	-0.043639	4.163678
212.561934	5930.688723	7.954765	-0.043673	4.166408
212.828467	5938.625345	7.959770	-0.043728	4.169095
213.098223	5946.696467	7.964774	-0.043783	4.171826
212.964695	5954.726338	7.969779	-0.043764	4.174536
213.021352	5962.760628	7.974784	-0.043780	4.177249
213.235681	5970.732016	7.979789	-0.043825	4.179940
213.485961	5978.753783	7.984794	-0.043877	4.182647
213.689873	5986.782367	7.989798	-0.043921	4.185353
213.744459	5994.779327	7.994803	-0.043936	4.188046
213.854701	6002.855793	7.999808	-0.043962	4.190764
214.020782	6010.921838	8.004813	-0.043999	4.193478
214.120282	6018.938600	8.009818	-0.044023	4.196173
214.417909	6026.883617	8.014822	-0.044083	4.198844
214.714857	6034.872933	8.019827	-0.044144	4.201528
214.596144	6042.861829	8.024832	-0.044127	4.204205
214.873668	6050.906861	8.029837	-0.044185	4.206904
214.958702	6058.947260	8.034842	-0.044206	4.209598
215.093710	6067.006251	8.039846	-0.044237	4.212297
215.242982	6074.979470	8.044851	-0.044270	4.214965
215.482094	6083.018627	8.049856	-0.044320	4.217655
215.576825	6090.990696	8.054861	-0.044343	4.220319
215.730117	6098.990423	8.059866	-0.044377	4.222991
215.994923	6107.001343	8.064870	-0.044431	4.225666
216.102861	6115.032378	8.069875	-0.044457	4.228345
216.297071	6123.055725	8.074880	-0.044499	4.231020
216.334188	6131.096304	8.079885	-0.044511	4.233698
216.610041	6139.139799	8.084890	-0.044568	4.236377
216.764955	6147.117786	8.089894	-0.044602	4.239032
216.808588	6155.160395	8.094899	-0.044616	4.241705
217.332393	6163.095794	8.099904	-0.044718	4.244346
217.256320	6171.222560	8.104909	-0.044710	4.247042
217.443597	6179.153182	8.109914	-0.044750	4.249675
217.729114	6187.234928	8.114918	-0.044809	4.252357
217.771864	6195.207918	8.119923	-0.044822	4.254998
217.954212	6203.289605	8.124928	-0.044862	4.257676
218.063737	6211.241580	8.129933	-0.044887	4.260308
218.230491	6219.264982	8.134938	-0.044924	4.262963
218.408101	6227.293171	8.139942	-0.044962	4.265617
218.583969	6235.347291	8.144947	-0.045001	4.268279
218.839268	6243.372256	8.149952	-0.045053	4.270930
218.838398	6251.472449	8.154957	-0.045059	4.273602
219.146047	6259.436132	8.159962	-0.045122	4.276229
219.488204	6267.450410	8.164966	-0.045191	4.278872
219.408816	6275.446412	8.169971	-0.045181	4.281504
219.638636	6283.408146	8.174976	-0.045229	4.284126
219.757650	6291.478319	8.179981	-0.045257	4.286780
220.078943	6299.458218	8.184986	-0.045322	4.289405
220.372700	6307.536065	8.189990	-0.045383	4.292061
220.371453	6315.549219	8.194995	-0.045388	4.294691
220.415478	6323.569997	8.200000	-0.045401	4.297322
220.353165	6331.560182	8.205005	-0.045395	4.299941
220.525249	6339.542923	8.210010	-0.045433	4.302557
220.792997	6347.611308	8.215014	-0.045488	4.305201
221.081134	6355.595525	8.220019	-0.045547	4.307816
221.342476	6363.637871	8.225024	-0.045601	4.310447
221.569352	6371.677446	8.230029	-0.045649	4.313076
221.539699	6379.700200	8.235034	-0.045649	4.315696
221.641007	6387.701874	8.240038	-0.045673	4.318309
222.037888	6395.657713	8.245043	-0.045752	4.320907
222.367459	6403.697613	8.250048	-0.045819	4.323530
222.190051	6411.734643	8.255053	-0.045792	4.326148
222.202924	6419.703224	8.260058	-0.045799	4.328742
222.478298	6427.793705	8.265062	-0.045856	4.331377
222.795706	6435.768283	8.270067	-0.045921	4.333973
222.915704	6443.789489	8.275072	-0.045948	4.336580
223.171320	6451.805965	8.280077	-0.046001	4.339186
223.197992	6459.837005	8.285082	-0.046012	4.341793
223.432865	6467.806936	8.290086	-0.046061	4.344380
223.409039	6475.893987	8.295091	-0.046062	4.347002
223.836239	6483.855240	8.300096	-0.046147	4.349585
223.765901	6491.945297	8.305101	-0.046139	4.352204
223.899377	6500.000408	8.310106	-0.046170	4.354812
224.341612	6508.014676	8.315110	-0.046257	4.357407
224.427615	6515.935622	8.320115	-0.046279	4.359968
224.462964	6523.964724	8.325120	-0.046291	4.362562
224.880850	6531.974793	8.330125	-0.046374	4.365151
224.797853	6539.953884	8.335130	-0.046364	4.367725
225.092063	6548.007020	8.340134	-0.046424	4.370324
225.054932	6556.025741	8.345139	-0.046423	4.372908
225.514327	6564.039991	8.350144	-0.046514	4.375492
225.593334	6572.028315	8.355149	-0.046534	4.378064
225.495800	6580.021667	8.360154	-0.046521	4.380635
225.798320	6588.088262	8.365158	-0.046583	4.383230
225.863510	6596.087204	8.370163	-0.046601	4.385801
226.177947	6604.132199	8.375168	-0.046665	4.388386
226.263301	6612.141293	8.380173	-0.046686	4.390957
226.408929	6620.167718	8.385178	-0.046718	4.393532
226.623446	6628.242562	8.390182	-0.046764	4.396122
226.603315	6636.172188	8.395187	-0.046765	4.398662
226.983331	6644.215821	8.400192	-0.046842	4.401240
227.297953	6652.207823	8.405197	-0.046906	4.403799
227.418236	6660.244864	8.410202	-0.046933	4.406370
227.574698	6668.282167	8.415206	-0.046968	4.408940
227.636134	6676.320844	8.420211	-0.046985	4.411508
227.907548	6684.337481	8.425216	-0.047041	4.414069
228.195938	6692.384076	8.430221	-0.047100	4.416637
228.295470	6700.339440	8.435226	-0.047124	4.419175
228.282473	6708.408907	8.440230	-0.047127	4.421746
228.164382	6716.347366	8.445235	-0.047110	4.424274
228.357591	6724.394663	8.450240	-0.047152	4.426837
228.625578	6732.402435	8.455245	-0.047207	4.429385
228.542215	6740.433695	8.460250	-0.047197	4.431939
229.043226	6748.534068	8.465254	-0.047296	4.434515
229.236592	6756.521691	8.470259	-0.047337	4.437052
229.273685	6764.457073	8.475264	-0.047350	4.439571
229.530095	6772.501336	8.480269	-0.047403	4.442124
229.805293	6780.477193	8.485274	-0.047459	4.444654
229.719276	6788.548188	8.490278	-0.047449	4.447211
229.891030	6796.512984	8.495283	-0.047486	4.449734
230.068494	6804.612554	8.500288	-0.047525	4.452298
230.259821	6812.614018	8.505293	-0.047566	4.454829
230.330131	6820.624571	8.510298	-0.047584	4.457362
230.536895	6828.586662	8.515302	-0.047628	4.459878
230.616574	6836.615185	8.520307	-0.047649	4.462414
230.721646	6844.619318	8.525312	-0.047674	4.464940
230.948512	6852.684057	8.530317	-0.047721	4.467484
231.090652	6860.651419	8.535322	-0.047753	4.469996
231.489909	6868.759242	8.540326	-0.047833	4.472552
231.361118	6876.715977	8.545331	-0.047814	4.475057
231.463163	6884.739151	8.550336	-0.047839	4.477582
231.677359	6892.740894	8.555341	-0.047884	4.480099
231.849314	6900.775487	8.560346	-0.047922	4.482625
232.241500	6908.732921	8.565351	-0.048000	4.485126
232.439508	6916.786415	8.570355	-0.048042	4.487655
232.605566	6924.799071	8.575360	-0.048079	4.490170
232.580595	6932.853972	8.580365	-0.048080	4.492696
232.695782	6940.827399	8.585370	-0.048106	4.495196
232.956145	6948.872768	8.590375	-0.048160	4.497717
233.069105	6956.831325	8.595379	-0.048187	4.500209
233.384436	6964.905340	8.600384	-0.048251	4.502736
233.680479	6972.891321	8.605389	-0.048311	4.505234
233.676907	6980.925346	8.610394	-0.048316	4.507745
233.835724	6988.918535	8.615399	-0.048351	4.510242
234.057557	6996.998742	8.620403	-0.048398	4.512766
234.342438	7005.030030	8.625408	-0.048456	4.515272
234.389315	7013.021652	8.630413	-0.048471	4.517765
234.290165	7020.952672	8.635418	-0.048458	4.520236
234.450523	7029.029480	8.640423	-0.048493	4.522753
234.592838	7036.969552	8.645427	-0.048525	4.525225
234.919228	7045.020154	8.650432	-0.048591	4.527731
234.898010	7053.028464	8.655437	-0.048592	4.530221
235.021244	7061.105555	8.660442	-0.048621	4.532732
235.065422	7069.097199	8.665447	-0.048635	4.535214
235.332261	7077.058701	8.670451	-0.048690	4.537687
235.538437	7085.076342	8.675456	-0.048733	4.540175
235.510870	7093.184384	8.680461	-0.048734	4.542689
235.713907	7101.096160	8.685466	-0.048777	4.545142
235.996809	7109.191311	8.690471	-0.048835	4.547650
235.994568	7117.174495	8.695475	-0.048840	4.550122
236.069862	7125.213115	8.700480	-0.048860	4.552610
236.192073	7133.245851	8.705485	-0.048888	4.555094
236.170885	7141.207905	8.710490	-0.048889	4.557555
236.528545	7149.261577	8.715495	-0.048961	4.560044
236.635125	7157.231831	8.720499	-0.048987	4.562505
236.997760	7165.233765	8.725504	-0.049060	4.564975
236.790942	7173.289902	8.730509	-0.049026	4.567459
236.968329	7181.277061	8.735514	-0.049065	4.569921
237.383960	7189.377278	8.740519	-0.049148	4.572417
237.287091	7197.352882	8.745523	-0.049135	4.574873
237.591955	7205.393449	8.750528	-0.049197	4.577348
237.935877	7213.382547	8.755533	-0.049267	4.579806
237.925413	7221.409497	8.760538	-0.049270	4.582273
238.032013	7229.426271	8.765543	-0.049296	4.584737
238.078869	7237.468892	8.770547	-0.049310	4.587206
238.399652	7245.429860	8.775552	-0.049375	4.589650
238.410580	7253.519960	8.780557	-0.049382	4.592132
238.380316	7261.522843	8.785562	-0.049382	4.594585
238.975079	7269.566829	8.790567	-0.049498	4.597050
239.130737	7277.489464	8.795571	-0.049533	4.599477
239.286839	7285.562243	8.800576	-0.049567	4.601948
239.439503	7293.494483	8.805581	-0.049601	4.604375
239.480504	7301.578115	8.810586	-0.049614	4.606846
239.632222	7309.571030	8.815591	-0.049648	4.609289
239.667060	7317.626558	8.820595	-0.049660	4.611749
239.875150	7325.629117	8.825600	-0.049704	4.614192
239.982345	7333.707636	8.830605	-0.049729	4.616657
240.152864	7341.635912	8.835610	-0.049767	4.619075
240.347581	7349.679085	8.840615	-0.049808	4.621526
240.427334	7357.611712	8.845619	-0.049829	4.623943
240.478979	7365.640812	8.850624	-0.049844	4.626387
240.980555	7373.692141	8.855629	-0.049942	4.628837
241.024628	7381.728852	8.860634	-0.049956	4.631281
241.042955	7389.793423	8.865639	-0.049965	4.633733
241.108040	7397.792465	8.870643	-0.049983	4.636163
241.209165	7405.726901	8.875648	-0.050007	4.638572
241.358495	7413.758217	8.880653	-0.050040	4.641009
241.345337	7421.761534	8.885658	-0.050043	4.643437
241.857074	7429.829062	8.890663	-0.050144	4.645883
241.932588	7437.775174	8.895667	-0.050163	4.648290
241.932877	7445.821123	8.900672	-0.050169	4.650727
242.008560	7453.921052	8.905677	-0.050188	4.653179
242.493637	7461.858376	8.910682	-0.050284	4.655579
242.657450	7469.913518	8.915687	-0.050320	4.658015
242.651985	7477.949595	8.920691	-0.050324	4.660444
242.759600	7485.923105	8.925696	-0.050350	4.662852
242.815959	7493.907820	8.930701	-0.050366	4.665262
243.027117	7501.917015	8.935706	-0.050410	4.667679
243.382547	7509.971474	8.940711	-0.050482	4.670107
243.362010	7518.084476	8.945715	-0.050484	4.672553
243.494768	7526.127836	8.950720	-0.050514	4.674976
243.455785	7534.084337	8.955725	-0.050512	4.677372
243.653917	7541.990116	8.960730	-0.050554	4.679751
244.070622	7550.045490	8.965735	-0.050637	4.682173
244.206079	7557.998717	8.970739	-0.050668	4.684564
244.387733	7566.016613	8.975744	-0.050707	4.686973
244.511656	7574.091396	8.980749	-0.050736	4.689398
244.521595	7582.105208	8.985754	-0.050743	4.691803
244.849626	7590.076254	8.990759	-0.050810	4.694194
244.961232	7598.152134	8.995763	-0.050836	4.696615
244.811053	7606.081461	9.000768	-0.050813	4.698992
244.903276	7614.179068	9.005773	-0.050836	4.701418
244.990842	7622.109812	9.010778	-0.050858	4.703792
245.374606	7630.198099	9.015783	-0.050934	4.706212
245.318670	7638.185063	9.020787	-0.050929	4.708600
245.470531	7646.212153	9.025792	-0.050963	4.711000
245.607952	7654.277777	9.030797	-0.050994	4.713409
245.780696	7662.296638	9.035802	-0.051032	4.715804
245.927817	7670.307927	9.040807	-0.051065	4.718194
245.993735	7678.286015	9.045811	-0.051082	4.720574
246.187703	7686.258806	9.050816	-0.051124	4.722951
246.290223	7694.326043	9.055821	-0.051148	4.725355
246.247720	7702.330067	9.060826	-0.051146	4.727739
246.671855	7710.343513	9.065831	-0.051230	4.730124
246.442232	7718.403240	9.070835	-0.051193	4.732523
247.006016	7726.428468	9.075840	-0.051303	4.734908
247.204446	7734.451204	9.080845	-0.051346	4.737292
247.216817	7742.383697	9.085850	-0.051354	4.739649
247.176511	7750.456315	9.090855	-0.051352	4.742046
247.412642	7758.448581	9.095859	-0.051401	4.744418
247.494625	7766.432774	9.100864	-0.051422	4.746786
247.860377	7774.487267	9.105869	-0.051495	4.749173
248.011510	7782.535158	9.110874	-0.051529	4.751558
248.137833	7790.553144	9.115879	-0.051558	4.753933
248.021354	7798.614607	9.120883	-0.051541	4.756320
248.181011	7806.517616	9.125888	-0.051577	4.758658
248.677431	7814.597499	9.130893	-0.051674	4.761046
248.666161	7822.540314	9.135898	-0.051678	4.763394
248.646704	7830.569390	9.140903	-0.051680	4.765766
248.888739	7838.588796	9.145907	-0.051730	4.768134
249.010827	7846.619240	9.150912	-0.051758	4.770504
249.207833	7854.689622	9.155917	-0.051800	4.772884
249.552575	7862.631543	9.160922	-0.051870	4.775224
249.797898	7870.707571	9.165927	-0.051921	4.777604
249.731812	7878.675429	9.170931	-0.051914	4.779951
249.820507	7886.650350	9.175936	-0.051936	4.782299
250.145818	7894.709955	9.180941	-0.052002	4.784669
250.091805	7902.686641	9.185946	-0.051998	4.787016
250.277974	7910.769415	9.190951	-0.052038	4.789391
250.374888	7918.739164	9.195955	-0.052061	4.791733
250.668266	7926.775259	9.200960	-0.052121	4.794092
250.782522	7934.835128	9.205965	-0.052148	4.796457
250.949137	7942.748681	9.210970	-0.052184	4.798779
251.120564	7950.829127	9.215975	-0.052222	4.801148
251.063876	7958.806799	9.220979	-0.052217	4.803486
251.296358	7966.816288	9.225984	-0.052265	4.805832
251.401404	7974.820317	9.230989	-0.052290	4.808175
251.454754	7982.833877	9.235994	-0.052306	4.810520
251.606758	7990.265886	9.240999	-0.052339	4.812694
251.738452	7994.735725	9.246003	-0.052367	4.814001

251.838978	7997.279761	9.251008	-0.052387	4.814744
251.887230	7998.590887	9.256013	-0.052397	4.815127
251.946604	7998.999837	9.261018	-0.052409	4.815246
252.275703	8000.048683	9.266023	-0.052471	4.815551
252.231422	8000.027684	9.271027	-0.052463	4.815545
252.358603	8000.068232	9.276032	-0.052487	4.815557
252.530932	8000.068932	9.281037	-0.052519	4.815556
252.789198	8000.045403	9.286042	-0.052567	4.815548
252.756481	8000.088677	9.291047	-0.052562	4.815561
252.977888	8000.057070	9.296051	-0.052603	4.815550
253.132216	8000.051068	9.301056	-0.052632	4.815548
253.292016	8000.091082	9.306061	-0.052662	4.815559
253.209143	8000.040614	9.311066	-0.052647	4.815544
253.281905	8000.067456	9.316071	-0.052660	4.815552
253.410280	8000.043940	9.321075	-0.052685	4.815544
253.294990	8000.048481	9.326080	-0.052663	4.815546
253.510316	8000.055226	9.331085	-0.052704	4.815547
253.351955	8000.030224	9.336090	-0.052674	4.815541
253.393921	8000.038406	9.341095	-0.052682	4.815543
253.486967	8000.055967	9.346099	-0.052700	4.815547
253.584460	8000.038355	9.351104	-0.052718	4.815542
253.319560	8000.070356	9.356109	-0.052669	4.815552
253.427744	8000.044373	9.361114	-0.052689	4.815544
253.609980	8000.029215	9.366119	-0.052724	4.815539
253.598852	7999.997009	9.371123	-0.052722	4.815530
253.469708	8000.007732	9.376128	-0.052698	4.815533
253.616219	8000.049666	9.381133	-0.052725	4.815545
253.661609	8000.022656	9.386138	-0.052734	4.815537
253.826469	8000.061687	9.391143	-0.052765	4.815547
253.650882	8000.063105	9.396147	-0.052733	4.815549
253.838491	8000.061920	9.401152	-0.052768	4.815547
253.828621	8000.067118	9.406157	-0.052766	4.815549
253.756279	8000.001867	9.411162	-0.052753	4.815530
254.017506	8000.090539	9.416167	-0.052802	4.815555
254.112667	8000.065411	9.421171	-0.052820	4.815547
254.034023	8000.041713	9.426176	-0.052805	4.815541
254.115786	8000.056954	9.431181	-0.052821	4.815545
254.067481	8000.040161	9.436186	-0.052812	4.815540
253.916044	8000.065473	9.441191	-0.052784	4.815548
253.840540	8000.065324	9.446195	-0.052770	4.815548
254.210213	8000.023326	9.451200	-0.052839	4.815534
254.153590	8000.077959	9.456205	-0.052829	4.815551
253.878006	8000.041426	9.461210	-0.052778	4.815541
254.010374	8000.119445	9.466215	-0.052802	4.815563
254.099505	8000.102764	9.471219	-0.052819	4.815558
254.163709	8000.104901	9.476224	-0.052831	4.815558
253.992747	8000.109599	9.481229	-0.052800	4.815561
254.334682	8000.036172	9.486234	-0.052864	4.815537
254.359029	8000.100676	9.491239	-0.052868	4.815556
254.473583	8000.058776	9.496243	-0.052890	4.815543
254.207302	8000.043757	9.501248	-0.052841	4.815540
254.384613	8000.080856	9.506253	-0.052874	4.815550
254.051122	8000.016672	9.511258	-0.052812	4.815533
254.461955	8000.049047	9.516263	-0.052889	4.815541
254.459952	8000.059713	9.521267	-0.052888	4.815544
254.295449	8000.052768	9.526272	-0.052858	4.815542
254.389027	8000.083156	9.531277	-0.052876	4.815551
254.304736	8000.041207	9.536282	-0.052860	4.815539
254.258314	8000.085327	9.541287	-0.052852	4.815552
254.208749	8000.062104	9.546291	-0.052843	4.815546
254.429235	8000.031551	9.551296	-0.052884	4.815536
254.695428	8000.108557	9.556301	-0.052934	4.815557
254.637868	8000.056364	9.561306	-0.052923	4.815542
254.665011	8000.100619	9.566311	-0.052929	4.815555
254.716947	8000.097215	9.571315	-0.052938	4.815553
254.578784	8000.065065	9.576320	-0.052913	4.815545
254.619714	8000.114887	9.581325	-0.052921	4.815559
254.628017	8000.085134	9.586330	-0.052922	4.815550
254.579379	8000.096106	9.591335	-0.052914	4.815554
254.754298	8000.082965	9.596339	-0.052946	4.815549
254.634256	8000.060725	9.601344	-0.052924	4.815543
254.890232	8000.085227	9.606349	-0.052972	4.815549
254.507184	8000.070431	9.611354	-0.052901	4.815547
254.711099	8000.088740	9.616359	-0.052939	4.815551
254.787574	8000.087874	9.621363	-0.052954	4.815550
254.765804	8000.102490	9.626368	-0.052950	4.815555
254.665753	8000.109416	9.631373	-0.052931	4.815557
254.754507	8000.080980	9.636378	-0.052948	4.815548
254.799770	8000.105238	9.641383	-0.052957	4.815555
254.699271	8000.105748	9.646387	-0.052938	4.815556
254.864220	8000.059332	9.651392	-0.052969	4.815542
254.909042	8000.112422	9.656397	-0.052978	4.815557
254.916263	8000.024973	9.661402	-0.052979	4.815531
255.053788	8000.066762	9.666407	-0.053005	4.815543
254.976405	8000.079400	9.671411	-0.052991	4.815547
255.065050	8000.066984	9.676416	-0.053008	4.815543
255.054462	8000.090328	9.681421	-0.053006	4.815550
255.139399	8000.052216	9.686426	-0.053022	4.815538
255.106644	8000.106173	9.691431	-0.053016	4.815554
255.023970	8000.103770	9.696435	-0.053001	4.815554
255.094988	8000.097474	9.701440	-0.053014	4.815552
255.214617	8000.080224	9.706445	-0.053037	4.815546
255.003428	8000.036197	9.711450	-0.052998	4.815534
255.158037	8000.114583	9.716455	-0.053027	4.815556
255.226960	8000.085822	9.721459	-0.053040	4.815547
255.243336	8000.092517	9.726464	-0.053043	4.815549
255.047783	8000.102152	9.731469	-0.053007	4.815553
255.157269	8000.018513	9.736474	-0.053027	4.815528
255.257804	8000.052220	9.741479	-0.053046	4.815537
255.306368	8000.046625	9.746483	-0.053055	4.815536
255.182744	8000.014712	9.751488	-0.053033	4.815527
255.278994	8000.090007	9.756493	-0.053051	4.815548
255.033720	8000.046490	9.761498	-0.053005	4.815537
255.071708	8000.090924	9.766503	-0.053013	4.815550
255.222447	8000.092341	9.771507	-0.053041	4.815549
255.211668	8000.035573	9.776512	-0.053039	4.815533
255.313374	8000.101344	9.781517	-0.053058	4.815552
255.464353	8000.049359	9.786522	-0.053087	4.815536
255.555543	8000.088255	9.791527	-0.053104	4.815547
255.455788	8000.085572	9.796531	-0.053085	4.815546
255.340884	8000.047393	9.801536	-0.053064	4.815536
255.370822	8000.101308	9.806541	-0.053070	4.815551
255.311092	8000.092872	9.811546	-0.053059	4.815549
255.448366	8000.086593	9.816551	-0.053085	4.815547
255.395287	8000.094287	9.821555	-0.053075	4.815549
255.202002	8000.122118	9.826560	-0.053039	4.815558
255.268473	8000.112543	9.831565	-0.053052	4.815555
255.114412	8000.049156	9.836570	-0.053023	4.815537
255.309196	8000.064112	9.841575	-0.053060	4.815541
255.455931	8000.109258	9.846579	-0.053088	4.815553
255.301043	8000.012745	9.851584	-0.053059	4.815526
255.419657	8000.068112	9.856589	-0.053081	4.815541
255.296067	8000.056494	9.861594	-0.053058	4.815538
255.279850	8000.078678	9.866599	-0.053056	4.815545
255.433699	8000.044898	9.871603	-0.053084	4.815534
255.512689	8000.073981	9.876608	-0.053099	4.815542
255.419083	8000.081013	9.881613	-0.053082	4.815545
255.389764	8000.051711	9.886618	-0.053077	4.815537
255.561738	8000.094066	9.891623	-0.053109	4.815548
255.416603	8000.077823	9.896627	-0.053082	4.815544
255.300991	8000.062063	9.901632	-0.053061	4.815540
255.549991	8000.125974	9.906637	-0.053108	4.815557
255.521379	8000.104161	9.911642	-0.053102	4.815551
255.473154	8000.079891	9.916647	-0.053094	4.815544
255.332333	8000.095762	9.921651	-0.053068	4.815550
255.575218	8000.073053	9.926656	-0.053113	4.815542
255.730845	8000.122618	9.931661	-0.053142	4.815556
255.565860	8000.088959	9.936666	-0.053112	4.815547
255.524748	8000.075487	9.941671	-0.053104	4.815543
255.433878	8000.124220	9.946675	-0.053088	4.815557
255.306542	8000.060202	9.951680	-0.053064	4.815539
255.546395	8000.102600	9.956685	-0.053109	4.815551
255.547442	8000.027866	9.961690	-0.053109	4.815529
255.434327	8000.069826	9.966695	-0.053089	4.815542
255.357464	8000.046156	9.971699	-0.053074	4.815535
255.527608	8000.064982	9.976704	-0.053106	4.815540
255.412801	8000.073802	9.981709	-0.053085	4.815543
255.452166	8000.046693	9.986714	-0.053093	4.815535
255.590844	8000.073549	9.991719	-0.053119	4.815542
255.431862	8000.113691	9.996723	-0.053089	4.815554
255.221339	8000.036561	10.001728	-0.053050	4.815533
255.374455	8000.114924	10.006733	-0.053079	4.815555
255.371508	8000.073237	10.011738	-0.053079	4.815543
255.395919	8000.104631	10.016743	-0.053084	4.815552
255.335018	8000.071608	10.021747	-0.053072	4.815542
255.289086	8000.073011	10.026752	-0.053064	4.815543
255.263034	8000.105715	10.031757	-0.053059	4.815553
255.299192	8000.074281	10.036762	-0.053066	4.815543
255.642931	8000.144016	10.041767	-0.053131	4.815562
255.531455	8000.099484	10.046771	-0.053110	4.815550
255.419762	8000.072038	10.051776	-0.053089	4.815542
255.623075	8000.135201	10.056781	-0.053128	4.815560
255.740525	8000.089076	10.061786	-0.053150	4.815546
255.680245	8000.073154	10.066791	-0.053139	4.815541
255.471073	8000.074020	10.071795	-0.053100	4.815542
255.499107	8000.028567	10.076800	-0.053105	4.815529
255.692805	8000.099050	10.081805	-0.053142	4.815549
255.326853	8000.072783	10.086810	-0.053074	4.815543
255.469292	8000.080474	10.091815	-0.053100	4.815544
255.580092	8000.085510	10.096819	-0.053121	4.815545
255.317595	8000.022484	10.101824	-0.053072	4.815528
255.581093	8000.105858	10.106829	-0.053122	4.815551
255.578509	8000.050291	10.111834	-0.053121	4.815535
255.402252	8000.078400	10.116839	-0.053089	4.815544
255.371133	8000.091795	10.121843	-0.053083	4.815548
255.557825	8000.008351	10.126848	-0.053118	4.815523
255.566773	8000.079013	10.131853	-0.053120	4.815543
255.588994	8000.054828	10.136858	-0.053124	4.815536
255.645952	8000.038688	10.141863	-0.053135	4.815531
255.731611	8000.056131	10.146867	-0.053151	4.815536
255.523929	8000.043136	10.151872	-0.053113	4.815533
255.567980	8000.091943	10.156877	-0.053121	4.815547
255.571429	7999.981999	10.161882	-0.053122	4.815515
255.588000	8000.052786	10.166887	-0.053126	4.815536
255.713137	8000.100783	10.171891	-0.053149	4.815549
255.576737	8000.066524	10.176896	-0.053124	4.815540
255.684311	8000.109962	10.181901	-0.053144	4.815552
255.400202	8000.098920	10.186906	-0.053091	4.815550
255.587343	8000.104138	10.191911	-0.053127	4.815551
255.590411	8000.088185	10.196915	-0.053127	4.815546
255.555456	8000.089767	10.201920	-0.053121	4.815547
255.478013	8000.104540	10.206925	-0.053107	4.815551
255.510178	8000.068768	10.211930	-0.053113	4.815541
255.691002	8000.089906	10.216935	-0.053147	4.815546
255.627526	8000.081408	10.221939	-0.053135	4.815544
255.552363	8000.073787	10.226944	-0.053121	4.815542
255.787246	8000.113968	10.231949	-0.053165	4.815552
255.520992	8000.091469	10.236954	-0.053116	4.815547
255.534235	8000.072477	10.241959	-0.053119	4.815542
255.764403	8000.060242	10.246963	-0.053162	4.815537
255.928375	8000.023424	10.251968	-0.053192	4.815525
255.759674	8000.070883	10.256973	-0.053161	4.815540
255.924115	8000.072526	10.261978	-0.053192	4.815540
255.923518	8000.047967	10.266983	-0.053192	4.815532
255.569217	8000.083842	10.271987	-0.053126	4.815545
255.570218	8000.044356	10.276992	-0.053127	4.815533
255.755639	8000.122180	10.281997	-0.053162	4.815555
255.726529	8000.100359	10.287002	-0.053156	4.815549
255.711147	8000.123625	10.292007	-0.053154	4.815556
255.821401	8000.097677	10.297011	-0.053174	4.815547
255.865893	8000.072788	10.302016	-0.053183	4.815540
255.786561	8000.081121	10.307021	-0.053168	4.815543
255.997159	8000.061089	10.312026	-0.053208	4.815536
255.841325	8000.070305	10.317031	-0.053179	4.815539
255.736851	8000.076090	10.322035	-0.053160	4.815542
255.871752	7999.999274	10.327040	-0.053185	4.815518
256.000228	8000.066554	10.332045	-0.053209	4.815537
255.664204	8000.074956	10.337050	-0.053147	4.815542
255.706630	8000.056442	10.342055	-0.053155	4.815536
256.087688	8000.092609	10.347059	-0.053226	4.815545
256.003060	8000.064537	10.352064	-0.053211	4.815537
256.043960	8000.078044	10.357069	-0.053218	4.815541
255.989945	8000.061155	10.362074	-0.053209	4.815536
255.863559	8000.069786	10.367079	-0.053185	4.815539
255.876851	8000.111680	10.372083	-0.053188	4.815551
255.859156	8000.077228	10.377088	-0.053185	4.815541
255.909213	8000.138951	10.382093	-0.053194	4.815559
255.937269	8000.094566	10.387098	-0.053200	4.815546
255.786161	8000.093178	10.392103	-0.053172	4.815546
255.874398	8000.114936	10.397107	-0.053189	4.815552
255.720116	8000.047271	10.402112	-0.053160	4.815533
255.788897	8000.103960	10.407117	-0.053173	4.815549
255.819643	8000.091664	10.412122	-0.053179	4.815546
256.103799	8000.088858	10.417127	-0.053232	4.815543
255.943687	8000.055279	10.422131	-0.053202	4.815534
255.889754	8000.044800	10.427136	-0.053193	4.815532
255.965848	8000.122972	10.432141	-0.053207	4.815554
255.880815	8000.083145	10.437146	-0.053191	4.815543
255.931419	8000.063697	10.442151	-0.053201	4.815537
255.974676	8000.077241	10.447155	-0.053209	4.815541
255.951135	8000.058716	10.452160	-0.053205	4.815535
256.135721	8000.098074	10.457165	-0.053240	4.815546
256.081171	8000.076904	10.462170	-0.053230	4.815540
255.989638	8000.038038	10.467175	-0.053213	4.815529
255.839488	8000.084733	10.472179	-0.053185	4.815543
255.857619	8000.031641	10.477184	-0.053189	4.815528
256.202237	8000.104597	10.482189	-0.053253	4.815547
256.119555	8000.089375	10.487194	-0.053238	4.815543
256.171079	8000.113737	10.492199	-0.053248	4.815550
256.164241	8000.106166	10.497203	-0.053247	4.815548
256.152335	8000.086763	10.502208	-0.053245	4.815542
255.910609	8000.084959	10.507213	-0.053200	4.815543
255.958739	8000.068675	10.512218	-0.053209	4.815538
255.930104	8000.083179	10.517223	-0.053204	4.815542
256.129304	8000.116368	10.522227	-0.053241	4.815551
255.990976	8000.048963	10.527232	-0.053216	4.815532
256.195558	8000.123899	10.532237	-0.053254	4.815553
256.288072	8000.128637	10.537242	-0.053271	4.815554
256.265160	8000.102644	10.542247	-0.053267	4.815547
256.344218	8000.134935	10.547251	-0.053282	4.815556
256.359541	8000.030524	10.552256	-0.053285	4.815525
256.354226	8000.104159	10.557261	-0.053285	4.815547
256.143378	8000.090042	10.562266	-0.053246	4.815543
256.407018	8000.050584	10.567271	-0.053295	4.815531
256.272856	8000.110358	10.572275	-0.053270	4.815549
255.990902	8000.104691	10.577280	-0.053218	4.815548
256.192946	8000.111223	10.582285	-0.053256	4.815549
256.197237	8000.097425	10.587290	-0.053257	4.815545
256.162945	8000.104359	10.592295	-0.053250	4.815547
256.128147	8000.113421	10.597299	-0.053244	4.815550
256.147075	8000.079569	10.602304	-0.053248	4.815540
256.328214	8000.130621	10.607309	-0.053282	4.815554
256.278079	8000.075342	10.612314	-0.053273	4.815538
256.208043	8000.092372	10.617319	-0.053260	4.815544
256.330497	8000.091192	10.622323	-0.053283	4.815543
256.179853	8000.084471	10.627328	-0.053255	4.815542
256.275100	8000.146934	10.632333	-0.053273	4.815559
256.256241	8000.123144	10.637338	-0.053270	4.815552
256.340882	8000.146981	10.642343	-0.053286	4.815559
256.394794	8000.147882	10.647347	-0.053296	4.815559
256.327055	8000.122223	10.652352	-0.053284	4.815552
256.250118	8000.119913	10.657357	-0.053269	4.815552
256.171279	8000.106891	10.662362	-0.053255	4.815548
256.223945	8000.119522	10.667367	-0.053265	4.815552
256.342454	8000.115072	10.672371	-0.053287	4.815550
256.105013	8000.101588	10.677376	-0.053243	4.815547
256.506867	8000.124211	10.682381	-0.053318	4.815552
256.478869	8000.099203	10.687386	-0.053313	4.815544
256.414009	8000.119523	10.692391	-0.053301	4.815551
256.198906	8000.145926	10.697395	-0.053262	4.815559
256.333590	8000.146015	10.702400	-0.053287	4.815559
256.311550	8000.162763	10.707405	-0.053283	4.815564
256.259286	8000.094631	10.712410	-0.053273	4.815544
256.187236	8000.110560	10.717415	-0.053260	4.815549
256.313695	8000.140422	10.722419	-0.053284	4.815557
256.207413	8000.086359	10.727424	-0.053264	4.815542
256.374383	8000.121158	10.732429	-0.053296	4.815551
256.399246	8000.060698	10.737434	-0.053301	4.815533
256.240987	8000.059192	10.742439	-0.053271	4.815534
256.327750	8000.112972	10.747443	-0.053288	4.815549
256.477965	8000.091951	10.752448	-0.053316	4.815542
256.445057	8000.137362	10.757453	-0.053310	4.815556
256.166198	8000.085814	10.762458	-0.053258	4.815542
256.269588	8000.119570	10.767463	-0.053278	4.815551
256.317483	8000.118237	10.772467	-0.053287	4.815551
256.305887	8000.047567	10.777472	-0.053285	4.815530
256.427503	8000.121144	10.782477	-0.053308	4.815551
256.184673	8000.097958	10.787482	-0.053263	4.815545
256.464506	8000.072651	10.792487	-0.053315	4.815537
256.382318	8000.133277	10.797491	-0.053300	4.815555
256.366734	8000.072155	10.802496	-0.053297	4.815537
256.554639	8000.106228	10.807501	-0.053332	4.815546
256.626634	8000.082858	10.812506	-0.053346	4.815539
256.493793	8000.094587	10.817511	-0.053322	4.815543
256.762698	8000.100078	10.822515	-0.053372	4.815543
256.564720	8000.069081	10.827520	-0.053335	4.815535
256.521764	8000.096169	10.832525	-0.053327	4.815543
256.508694	8000.087428	10.837530	-0.053325	4.815541
256.570271	8000.054273	10.842535	-0.053337	4.815531
256.775522	8000.124949	10.847539	-0.053375	4.815550
256.479205	8000.091273	10.852544	-0.053320	4.815542
256.718456	8000.163574	10.857549	-0.053365	4.815562
256.600812	8000.144574	10.862554	-0.053343	4.815557
256.579041	8000.121804	10.867559	-0.053340	4.815550
256.742007	8000.140515	10.872563	-0.053370	4.815555
256.535320	8000.097625	10.877568	-0.053332	4.815543
256.443814	8000.103622	10.882573	-0.053315	4.815546
256.464153	8000.085815	10.887578	-0.053319	4.815540
256.600499	8000.097680	10.892583	-0.053345	4.815543
256.677161	8000.110704	10.897587	-0.053359	4.815547
256.678133	8000.079761	10.902592	-0.053359	4.815537
256.537354	8000.113792	10.907597	-0.053333	4.815548
256.366433	8000.106738	10.912602	-0.053302	4.815547
256.383782	8000.127336	10.917607	-0.053305	4.815553
256.456949	8000.113598	10.922611	-0.053319	4.815548
256.454332	8000.082597	10.927616	-0.053319	4.815539
256.307774	8000.098374	10.932621	-0.053292	4.815545
256.442612	8000.099533	10.937626	-0.053317	4.815544
256.635349	8000.123004	10.942631	-0.053353	4.815550
256.704197	8000.138036	10.947635	-0.053366	4.815554
256.605553	8000.109734	10.952640	-0.053348	4.815547
256.702675	8000.123094	10.957645	-0.053366	4.815550
256.657133	8000.103139	10.962650	-0.053358	4.815544
256.480149	8000.091713	10.967655	-0.053325	4.815542
256.612693	8000.134493	10.972659	-0.053350	4.815554
256.779278	8000.114809	10.977664	-0.053381	4.815547
256.816723	8000.119714	10.982669	-0.053389	4.815548
256.593970	8000.086174	10.987674	-0.053347	4.815540
256.804712	8000.092849	10.992679	-0.053387	4.815541
256.818168	8000.095224	10.997683	-0.053389	4.815541
256.681910	8000.087670	11.002688	-0.053364	4.815540
256.695644	8000.153072	11.007693	-0.053367	4.815559
256.701769	8000.101918	11.012698	-0.053368	4.815544
256.544564	8000.120725	11.017703	-0.053339	4.815550
256.710681	8000.129874	11.022707	-0.053371	4.815552
256.677908	8000.114401	11.027712	-0.053365	4.815547
256.488571	8000.136954	11.032717	-0.053330	4.815555
256.628439	8000.123241	11.037722	-0.053356	4.815550
256.577631	8000.155541	11.042727	-0.053347	4.815560
256.562645	8000.132882	11.047731	-0.053344	4.815553
256.428688	8000.096525	11.052736	-0.053319	4.815543
256.852088	8000.078911	11.057741	-0.053398	4.815536
256.843532	8000.098016	11.062746	-0.053397	4.815542
256.656515	8000.093903	11.067751	-0.053362	4.815542
256.648999	8000.115162	11.072755	-0.053361	4.815548
256.609509	8000.117738	11.077760	-0.053354	4.815549
256.482902	8000.099660	11.082765	-0.053331	4.815544
256.462396	8000.112161	11.087770	-0.053327	4.815548
256.612488	8000.096479	11.092775	-0.053355	4.815542
256.757980	8000.122381	11.097779	-0.053382	4.815549
256.501407	8000.073333	11.102784	-0.053335	4.815536
256.693699	8000.126705	11.107789	-0.053371	4.815551
256.749770	8000.109483	11.112794	-0.053382	4.815546
256.864833	8000.116728	11.117799	-0.053403	4.815547
256.948157	8000.120248	11.122803	-0.053419	4.815548
256.797217	8000.093225	11.127808	-0.053391	4.815541
256.759792	8000.141767	11.132813	-0.053384	4.815555
256.499492	8000.124703	11.137818	-0.053336	4.815551
256.607680	8000.075221	11.142823	-0.053356	4.815536
256.810667	8000.134110	11.147827	-0.053394	4.815552
256.570972	8000.090679	11.152832	-0.053350	4.815541
256.657821	8000.157279	11.157837	-0.053366	4.815560
256.625467	8000.119382	11.162842	-0.053361	4.815549
256.705965	8000.106833	11.167847	-0.053376	4.815545
256.671369	8000.140466	11.172851	-0.053370	4.815555
256.607792	8000.100989	11.177856	-0.053358	4.815544
256.431397	8000.138708	11.182861	-0.053325	4.815556
256.448719	8000.121920	11.187866	-0.053329	4.815551
256.556956	8000.110893	11.192871	-0.053349	4.815547
256.663946	8000.141505	11.197875	-0.053369	4.815555
256.378789	8000.130443	11.202880	-0.053316	4.815553
256.736363	8000.117092	11.207885	-0.053383	4.815548
256.640059	8000.116601	11.212890	-0.053365	4.815548
256.743737	8000.068113	11.217895	-0.053385	4.815533
256.777841	8000.107145	11.222899	-0.053391	4.815545
256.664797	8000.121334	11.227904	-0.053371	4.815549
256.519257	8000.123241	11.232909	-0.053344	4.815551
256.718378	8000.119044	11.237914	-0.053381	4.815548
256.757455	8000.091930	11.242919	-0.053388	4.815540
256.979409	8000.143654	11.247923	-0.053430	4.815554
256.810708	8000.138772	11.252928	-0.053399	4.815554
256.762213	8000.176450	11.257933	-0.053390	4.815565
256.826300	8000.144405	11.262938	-0.053402	4.815555
256.911877	8000.140485	11.267943	-0.053418	4.815554
256.839644	8000.133979	11.272947	-0.053405	4.815552
256.784416	8000.036956	11.277952	-0.053395	4.815524
257.054706	8000.125789	11.282957	-0.053446	4.815549
256.873330	8000.134586	11.287962	-0.053412	4.815552
256.809075	8000.131415	11.292967	-0.053400	4.815552
257.037267	8000.137309	11.297971	-0.053443	4.815552
256.796772	8000.083183	11.302976	-0.053398	4.815537
257.040659	8000.103219	11.307981	-0.053444	4.815542
257.024053	8000.139284	11.312986	-0.053441	4.815553
256.821330	8000.101799	11.317991	-0.053404	4.815543
256.861152	8000.146266	11.322995	-0.053411	4.815556
256.731360	8000.132408	11.328000	-0.053387	4.815552
256.835933	8000.157640	11.333005	-0.053407	4.815559
256.821135	8000.096529	11.338010	-0.053404	4.815541
256.954094	8000.110476	11.343015	-0.053429	4.815545
257.058656	8000.161344	11.348019	-0.053449	4.815559
256.867702	8000.114438	11.353024	-0.053414	4.815546
256.771241	8000.136377	11.358029	-0.053396	4.815553
256.960508	8000.133087	11.363034	-0.053431	4.815551
257.069119	8000.134885	11.368039	-0.053452	4.815551
257.013128	8000.166032	11.373043	-0.053442	4.815561
257.167041	8000.144004	11.378048	-0.053470	4.815553
257.045176	8000.140957	11.383053	-0.053448	4.815553
256.992321	8000.144382	11.388058	-0.053438	4.815554
257.018119	8000.086073	11.393063	-0.053443	4.815537
257.087476	8000.127819	11.398067	-0.053456	4.815549
256.869705	8000.123201	11.403072	-0.053416	4.815549
256.840337	8000.107784	11.408077	-0.053411	4.815544
257.045936	8000.116512	11.413082	-0.053449	4.815546
256.896651	8000.080971	11.418087	-0.053422	4.815536
256.880707	8000.167251	11.423091	-0.053419	4.815562
256.741159	8000.134006	11.428096	-0.053393	4.815552
256.740597	8000.099833	11.433101	-0.053393	4.815542
256.820376	8000.097954	11.438106	-0.053408	4.815542
257.032169	8000.066193	11.443111	-0.053448	4.815531
257.065700	8000.141534	11.448115	-0.053454	4.815553
257.147126	8000.073454	11.453120	-0.053470	4.815533
257.111396	8000.146592	11.458125	-0.053463	4.815554
257.216235	8000.125897	11.463130	-0.053483	4.815548
257.199513	8000.120300	11.468135	-0.053480	4.815546
256.996374	8000.126604	11.473139	-0.053443	4.815549
256.997339	8000.105274	11.478144	-0.053443	4.815543
257.137288	8000.105449	11.483149	-0.053469	4.815542
256.909192	8000.109208	11.488154	-0.053427	4.815544
256.983410	8000.094420	11.493159	-0.053441	4.815540
257.196168	8000.116083	11.498163	-0.053481	4.815545
257.062530	8000.116048	11.503168	-0.053456	4.815546
257.082595	8000.071532	11.508173	-0.053460	4.815532
256.973795	8000.093268	11.513178	-0.053440	4.815539
257.147853	8000.123911	11.518183	-0.053473	4.815547
257.217192	8000.148566	11.523187	-0.053486	4.815554
257.009184	8000.123812	11.528192	-0.053447	4.815548
257.000587	8000.139713	11.533197	-0.053446	4.815553
256.908451	8000.138222	11.538202	-0.053429	4.815553
256.898907	8000.065447	11.543207	-0.053427	4.815532
257.174923	8000.157580	11.548211	-0.053479	4.815557
257.091979	8000.157307	11.553216	-0.053464	4.815557
257.076343	8000.170956	11.558221	-0.053461	4.815562
256.862598	8000.138631	11.563226	-0.053422	4.815553
256.921906	8000.124666	11.568231	-0.053433	4.815549
257.049117	8000.141724	11.573235	-0.053457	4.815553
256.762923	8000.119962	11.578240	-0.053404	4.815548
256.886043	8000.130543	11.583245	-0.053427	4.815551
256.990605	8000.106638	11.588250	-0.053446	4.815543
256.879716	8000.088817	11.593255	-0.053426	4.815538
256.929826	8000.120634	11.598259	-0.053435	4.815547
256.971265	8000.114923	11.603264	-0.053443	4.815546
256.937152	8000.085541	11.608269	-0.053437	4.815537
256.991752	8000.084318	11.613274	-0.053448	4.815537
257.085218	8000.057026	11.618279	-0.053465	4.815528
257.148052	8000.128575	11.623283	-0.053477	4.815549
256.955467	8000.106211	11.628288	-0.053442	4.815543
257.194171	8000.132572	11.633293	-0.053486	4.815550
257.300335	8000.137535	11.638298	-0.053506	4.815551
257.155850	8000.077504	11.643303	-0.053479	4.815534
257.110080	8000.152614	11.648307	-0.053471	4.815556
257.118226	8000.092947	11.653312	-0.053473	4.815538
257.161824	8000.128930	11.658317	-0.053481	4.815549
257.033050	8000.078770	11.663322	-0.053457	4.815535
257.147978	8000.057171	11.668327	-0.053479	4.815528
257.145066	8000.132984	11.673331	-0.053479	4.815550
257.000473	8000.118883	11.678336	-0.053452	4.815547
257.260263	8000.139181	11.683341	-0.053501	4.815551
257.300919	8000.132388	11.688346	-0.053508	4.815549
257.163949	8000.095980	11.693351	-0.053483	4.815539
257.174300	8000.125010	11.698355	-0.053485	4.815547
257.195889	8000.049540	11.703360	-0.053489	4.815525
257.157408	8000.070292	11.708365	-0.053482	4.815532
257.075411	8000.106354	11.713370	-0.053467	4.815542
257.242291	8000.099493	11.718375	-0.053499	4.815540
257.324661	8000.113679	11.723379	-0.053514	4.815543
257.050716	8000.087845	11.728384	-0.053463	4.815537
257.431220	8000.087689	11.733389	-0.053534	4.815535
257.454216	8000.126540	11.738394	-0.053539	4.815547
257.316206	8000.080501	11.743399	-0.053513	4.815534
257.152292	8000.152607	11.748403	-0.053483	4.815556
257.181316	8000.085805	11.753408	-0.053489	4.815536
257.415190	8000.137724	11.758413	-0.053533	4.815550
257.257181	8000.176813	11.763418	-0.053503	4.815562
257.208453	8000.101259	11.768423	-0.053494	4.815540
257.489529	8000.140066	11.773427	-0.053547	4.815550
257.280650	8000.109957	11.778432	-0.053508	4.815542
257.182317	8000.112637	11.783437	-0.053490	4.815544
257.295493	8000.104896	11.788442	-0.053512	4.815541
257.519846	8000.100045	11.793447	-0.053554	4.815538
257.260264	8000.139606	11.798451	-0.053505	4.815551
257.176553	8000.111548	11.803456	-0.053490	4.815543
257.211888	8000.135646	11.808461	-0.053497	4.815550
256.993057	8000.111783	11.813466	-0.053456	4.815544
256.961163	8000.084574	11.818471	-0.053451	4.815537
257.459388	8000.103438	11.823475	-0.053544	4.815540
257.257122	8000.115097	11.828480	-0.053506	4.815544
257.054409	8000.111794	11.833485	-0.053469	4.815544
257.358729	8000.096503	11.838490	-0.053525	4.815538
257.430025	8000.070985	11.843495	-0.053539	4.815530
257.352635	8000.138100	11.848499	-0.053525	4.815550
257.156958	8000.100730	11.853504	-0.053488	4.815540
257.380697	8000.091596	11.858509	-0.053530	4.815537
257.137851	8000.072681	11.863514	-0.053485	4.815532
257.147311	8000.056831	11.868519	-0.053487	4.815528
257.379900	8000.116207	11.873523	-0.053531	4.815544
257.139255	8000.112282	11.878528	-0.053486	4.815544
257.340738	8000.099579	11.883533	-0.053524	4.815539
257.515387	8000.103528	11.888538	-0.053557	4.815539
257.219515	8000.069857	11.893543	-0.053502	4.815531
257.213893	8000.111443	11.898547	-0.053501	4.815543
257.134871	8000.053552	11.903552	-0.053486	4.815527
257.098786	8000.086093	11.908557	-0.053480	4.815536
257.299980	8000.125727	11.913562	-0.053518	4.815547
257.073567	8000.015216	11.918567	-0.053476	4.815516
257.513827	8000.105768	11.923571	-0.053558	4.815540
257.353613	8000.086070	11.928576	-0.053528	4.815535
257.437109	8000.107753	11.933581	-0.053544	4.815541
257.378412	8000.118559	11.938586	-0.053533	4.815544
257.317758	8000.104765	11.943591	-0.053522	4.815541
257.302462	8000.140852	11.948595	-0.053520	4.815551
257.298943	8000.105562	11.953600	-0.053519	4.815541
257.386480	8000.102742	11.958605	-0.053536	4.815540
257.373875	8000.155964	11.963610	-0.053534	4.815555
257.297046	8000.070336	11.968615	-0.053519	4.815531
257.408497	8000.121318	11.973619	-0.053540	4.815545
257.311467	8000.118678	11.978624	-0.053522	4.815545
257.287013	8000.181320	11.983629	-0.053518	4.815563
257.345285	8000.156656	11.988634	-0.053529	4.815556
257.386963	8000.037720	11.993639	-0.053537	4.815521
257.243616	8000.109095	11.998643	-0.053511	4.815542
257.129899	8000.098704	12.003648	-0.053490	4.815540
257.325274	8000.101924	12.008653	-0.053526	4.815540
257.616447	8000.130215	12.013658	-0.053581	4.815547
257.324287	8000.128650	12.018663	-0.053527	4.815547
257.725659	8000.176907	12.023667	-0.053602	4.815560
257.582560	8000.162830	12.028672	-0.053575	4.815556
257.479033	8000.130173	12.033677	-0.053556	4.815547
257.518065	8000.145786	12.038682	-0.053563	4.815552
257.461759	8000.132064	12.043687	-0.053553	4.815548
257.468513	8000.163171	12.048691	-0.053555	4.815557
257.373492	8000.132790	12.053696	-0.053537	4.815548
257.449268	8000.137255	12.058701	-0.053552	4.815549
257.350059	8000.158080	12.063706	-0.053533	4.815556
257.370510	8000.115706	12.068711	-0.053537	4.815543
257.624297	8000.181840	12.073715	-0.053585	4.815562
257.647607	8000.160876	12.078720	-0.053589	4.815555
257.730119	8000.156906	12.083725	-0.053605	4.815554
257.333759	8000.157905	12.088730	-0.053531	4.815556
257.205585	8000.146209	12.093735	-0.053508	4.815553
257.432781	8000.159565	12.098739	-0.053550	4.815556
257.582547	8000.132129	12.103744	-0.053578	4.815547
257.743193	8000.110211	12.108749	-0.053608	4.815540
257.457601	8000.118367	12.113754	-0.053555	4.815544
257.255413	8000.130027	12.118759	-0.053518	4.815548
257.421848	8000.168024	12.123763	-0.053549	4.815558
257.454219	8000.110890	12.128768	-0.053555	4.815542
257.454764	8000.126941	12.133773	-0.053556	4.815546
257.455388	8000.128037	12.138778	-0.053556	4.815547
257.420942	8000.103991	12.143783	-0.053550	4.815540
257.399826	8000.126096	12.148787	-0.053546	4.815546
257.249425	8000.102285	12.153792	-0.053518	4.815540
257.532799	8000.150744	12.158797	-0.053571	4.815553
257.471876	8000.124127	12.163802	-0.053560	4.815545
257.196033	8000.101466	12.168807	-0.053509	4.815540
257.481387	8000.183071	12.173811	-0.053562	4.815562
257.466124	8000.142248	12.178816	-0.053560	4.815551
257.413003	8000.094395	12.183821	-0.053550	4.815537
257.382472	8000.141982	12.188826	-0.053545	4.815551
257.466626	8000.087833	12.193831	-0.053560	4.815535
257.657061	8000.110200	12.198835	-0.053596	4.815540
257.321748	8000.110064	12.203840	-0.053534	4.815542
257.549599	8000.071089	12.208845	-0.053576	4.815529
257.507137	8000.084298	12.213850	-0.053569	4.815533
257.474027	8000.052796	12.218855	-0.053563	4.815524
257.502921	8000.083198	12.223859	-0.053568	4.815533
257.258429	8000.085619	12.228864	-0.053523	4.815535
257.545548	8000.096752	12.233869	-0.053577	4.815537
257.660855	8000.154207	12.238874	-0.053598	4.815553
257.531527	8000.112582	12.243879	-0.053575	4.815542
257.596233	8000.143571	12.248883	-0.053587	4.815550
257.492743	8000.122665	12.253888	-0.053568	4.815545
257.499665	8000.113184	12.258893	-0.053569	4.815542
257.634604	8000.130369	12.263898	-0.053595	4.815546
257.542502	8000.096831	12.268903	-0.053578	4.815537
257.677726	8000.144999	12.273907	-0.053603	4.815550
257.589404	8000.146774	12.278912	-0.053587	4.815551
257.683083	8000.140851	12.283917	-0.053605	4.815549
257.453193	8000.132829	12.288922	-0.053562	4.815548
257.547317	8000.111957	12.293927	-0.053580	4.815541
257.384462	8000.136012	12.298931	-0.053550	4.815549
257.415785	8000.123725	12.303936	-0.053556	4.815545
257.581579	8000.112574	12.308941	-0.053587	4.815541
257.803679	8000.137598	12.313946	-0.053628	4.815547
257.481371	8000.112037	12.318951	-0.053568	4.815542
257.734450	8000.140773	12.323955	-0.053616	4.815549
257.763254	8000.122035	12.328960	-0.053621	4.815543
257.758365	8000.111292	12.333965	-0.053621	4.815540
257.674104	8000.143044	12.338970	-0.053605	4.815550
257.503022	8000.054801	12.343975	-0.053573	4.815525
257.674558	8000.109973	12.348979	-0.053606	4.815540
257.617029	8000.131481	12.353984	-0.053595	4.815547
257.549421	8000.098346	12.358989	-0.053583	4.815537
257.601372	8000.098147	12.363994	-0.053593	4.815537
257.526344	8000.111891	12.368999	-0.053579	4.815541
257.595139	8000.149356	12.374003	-0.053592	4.815552
257.797516	8000.098213	12.379008	-0.053630	4.815536
257.791725	8000.068227	12.384013	-0.053629	4.815527
257.846016	8000.103318	12.389018	-0.053639	4.815537
257.786323	8000.084198	12.394023	-0.053628	4.815532
257.731197	8000.160224	12.399027	-0.053618	4.815554
257.705358	8000.139523	12.404032	-0.053614	4.815548
257.792570	8000.162336	12.409037	-0.053630	4.815555
257.731328	8000.181646	12.414042	-0.053619	4.815561
257.740298	8000.126265	12.419047	-0.053621	4.815544
257.685519	8000.170250	12.424051	-0.053611	4.815557
257.600996	8000.149655	12.429056	-0.053595	4.815552
257.613610	8000.138130	12.434061	-0.053598	4.815548
257.713228	8000.134441	12.439066	-0.053617	4.815547
257.635793	8000.102212	12.444071	-0.053602	4.815538
257.817841	8000.170375	12.449075	-0.053637	4.815557
257.671213	8000.131671	12.454080	-0.053609	4.815546
257.849698	8000.132479	12.459085	-0.053643	4.815546
257.615280	8000.130791	12.464090	-0.053599	4.815546
257.495440	8000.095731	12.469095	-0.053577	4.815537
257.888088	8000.113936	12.474099	-0.053651	4.815540
257.747418	8000.109512	12.479104	-0.053625	4.815539
257.965408	8000.118445	12.484109	-0.053665	4.815541
257.763239	8000.124763	12.489114	-0.053628	4.815544
257.508458	8000.109923	12.494119	-0.053581	4.815541
257.853829	8000.132694	12.499123	-0.053645	4.815546
257.603094	8000.107239	12.504128	-0.053599	4.815539
257.342697	8000.088034	12.509133	-0.053551	4.815535
257.828591	8000.171860	12.514138	-0.053641	4.815557
257.678747	8000.116011	12.519143	-0.053614	4.815542
257.693731	8000.116276	12.524147	-0.053617	4.815542
257.790980	8000.100797	12.529152	-0.053635	4.815537
257.888622	8000.115234	12.534157	-0.053653	4.815540
257.649451	8000.146583	12.539162	-0.053609	4.815551
257.708472	8000.095227	12.544167	-0.053620	4.815535
257.891605	8000.152726	12.549171	-0.053654	4.815551
257.666450	8000.131962	12.554176	-0.053613	4.815546
257.577047	8000.120902	12.559181	-0.053596	4.815543
257.661777	8000.089194	12.564186	-0.053612	4.815534
257.712774	8000.099663	12.569191	-0.053622	4.815537
257.700996	8000.141148	12.574195	-0.053620	4.815549
257.797028	8000.106422	12.579200	-0.053638	4.815538
257.932150	8000.123610	12.584205	-0.053663	4.815542
257.866841	8000.144991	12.589210	-0.053652	4.815549
257.802257	8000.131132	12.594215	-0.053640	4.815545
257.765045	8000.148700	12.599219	-0.053633	4.815551
257.882851	8000.135695	12.604224	-0.053655	4.815546
257.916375	8000.130922	12.609229	-0.053662	4.815545
257.907059	8000.164970	12.614234	-0.053660	4.815555
257.880670	8000.144260	12.619239	-0.053655	4.815549
257.806790	8000.166568	12.624243	-0.053642	4.815556
257.799589	8000.150445	12.629248	-0.053641	4.815551
257.988381	8000.095875	12.634253	-0.053676	4.815534
257.977650	8000.167288	12.639258	-0.053674	4.815555
257.755114	8000.109180	12.644263	-0.053633	4.815539
257.823233	8000.153043	12.649267	-0.053646	4.815552
257.827962	8000.111479	12.654272	-0.053647	4.815539
257.598675	8000.118421	12.659277	-0.053605	4.815542
257.883362	8000.143402	12.664282	-0.053658	4.815548
257.798506	8000.135620	12.669287	-0.053642	4.815547
257.936035	8000.109052	12.674291	-0.053668	4.815538
257.696935	8000.112628	12.679296	-0.053624	4.815540
258.039113	8000.134279	12.684301	-0.053688	4.815545
257.934228	8000.160352	12.689306	-0.053668	4.815553
257.860584	8000.122844	12.694311	-0.053655	4.815542
257.913751	8000.156848	12.699315	-0.053665	4.815552
257.971383	8000.157812	12.704320	-0.053676	4.815552
257.886534	8000.140416	12.709325	-0.053660	4.815547
257.781529	8000.148327	12.714330	-0.053641	4.815550
257.863280	8000.129390	12.719335	-0.053656	4.815544
257.789588	8000.188020	12.724339	-0.053643	4.815562
257.647431	8000.114138	12.729344	-0.053617	4.815541
257.795225	8000.156103	12.734349	-0.053644	4.815552
257.958629	8000.132095	12.739354	-0.053675	4.815545
257.573321	8000.104433	12.744359	-0.053603	4.815538
257.649265	8000.158039	12.749363	-0.053618	4.815554
257.780719	8000.137779	12.754368	-0.053642	4.815547
257.631789	8000.060582	12.759373	-0.053615	4.815525
257.735351	8000.119981	12.764378	-0.053634	4.815542
257.796906	8000.138100	12.769383	-0.053646	4.815547
257.980645	8000.172109	12.774387	-0.053681	4.815556
257.836854	8000.138792	12.779392	-0.053654	4.815547
258.079779	8000.134247	12.784397	-0.053699	4.815545
258.002584	8000.168252	12.789402	-0.053685	4.815555
257.781186	8000.136867	12.794407	-0.053644	4.815547
257.896492	8000.149458	12.799411	-0.053666	4.815550
258.117356	8000.130664	12.804416	-0.053707	4.815543
257.779308	8000.126209	12.809421	-0.053644	4.815544
257.803071	8000.147982	12.814426	-0.053649	4.815550
257.898553	8000.113246	12.819431	-0.053667	4.815539
257.807971	8000.109643	12.824435	-0.053650	4.815539
257.750094	8000.118327	12.829440	-0.053640	4.815542
258.012020	8000.126912	12.834445	-0.053689	4.815543
257.979423	8000.143488	12.839450	-0.053683	4.815548
258.027223	8000.101561	12.844455	-0.053692	4.815535
257.995068	8000.156600	12.849459	-0.053686	4.815552
258.123543	8000.149111	12.854464	-0.053710	4.815549
257.978052	8000.137130	12.859469	-0.053684	4.815546
257.819205	8000.168727	12.864474	-0.053654	4.815556
257.861587	8000.103211	12.869479	-0.053662	4.815537
258.093615	8000.150830	12.874483	-0.053706	4.815549
257.934236	8000.109780	12.879488	-0.053676	4.815538
257.985869	8000.125600	12.884493	-0.053686	4.815542
258.092347	8000.145524	12.889498	-0.053706	4.815548
257.749197	8000.093983	12.894503	-0.053642	4.815534
257.622654	8000.169907	12.899507	-0.053619	4.815557
257.803306	8000.142977	12.904512	-0.053653	4.815548
257.813092	8000.123928	12.909517	-0.053655	4.815543
257.956653	8000.147664	12.914522	-0.053682	4.815549
258.038079	8000.131926	12.919527	-0.053697	4.815544
257.974854	8000.164023	12.924531	-0.053686	4.815554
257.849362	8000.126733	12.929536	-0.053663	4.815543
257.849485	8000.113935	12.934541	-0.053663	4.815540
257.862698	8000.140875	12.939546	-0.053665	4.815547
257.756413	8000.155175	12.944551	-0.053646	4.815552
257.742947	8000.147495	12.949555	-0.053644	4.815550
257.703845	8000.136190	12.954560	-0.053637	4.815547
257.823814	8000.126425	12.959565	-0.053659	4.815543
257.752857	8000.181896	12.964570	-0.053646	4.815560
257.808427	8000.105914	12.969575	-0.053657	4.815537
257.911230	8000.150346	12.974579	-0.053676	4.815550
257.855336	8000.146244	12.979584	-0.053666	4.815549
258.003609	8000.111305	12.984589	-0.053694	4.815538
257.893600	8000.156522	12.989594	-0.053673	4.815552
257.754583	8000.128624	12.994599	-0.053648	4.815544
257.898919	8000.095758	12.999603	-0.053675	4.815534
258.020894	8000.111663	13.004608	-0.053698	4.815538
258.049762	8000.112154	13.009613	-0.053703	4.815538
257.997813	8000.141231	13.014618	-0.053694	4.815547
257.817297	8000.113722	13.019623	-0.053660	4.815540
257.994169	8000.133731	13.024627	-0.053694	4.815545
257.783104	8000.136699	13.029632	-0.053654	4.815547
257.766603	8000.105468	13.034637	-0.053652	4.815537
257.947091	8000.133015	13.039642	-0.053685	4.815545
258.112534	8000.095153	13.044647	-0.053716	4.815533
257.860347	8000.080355	13.049651	-0.053670	4.815530
258.072151	8000.105210	13.054656	-0.053709	4.815536
258.027177	8000.079922	13.059661	-0.053701	4.815529
258.164313	8000.098212	13.064666	-0.053727	4.815533
258.024855	8000.106627	13.069671	-0.053701	4.815537
258.152537	8000.086306	13.074675	-0.053725	4.815530
258.012323	8000.071207	13.079680	-0.053699	4.815526
257.894665	8000.108821	13.084685	-0.053677	4.815538
258.184494	8000.154183	13.089690	-0.053732	4.815550
258.144973	8000.105484	13.094695	-0.053725	4.815536
258.111336	8000.164771	13.099699	-0.053718	4.815553
258.082148	8000.165380	13.104704	-0.053713	4.815553
258.095690	8000.143187	13.109709	-0.053716	4.815547
258.101183	8000.167865	13.114714	-0.053717	4.815554
258.058227	8000.112700	13.119719	-0.053709	4.815538
258.232929	8000.168994	13.124723	-0.053742	4.815554
258.017320	8000.175091	13.129728	-0.053702	4.815557
257.822295	8000.123843	13.134733	-0.053666	4.815542
257.832907	8000.152877	13.139738	-0.053668	4.815551
257.883496	8000.085359	13.144743	-0.053678	4.815531
257.846543	8000.163820	13.149747	-0.053671	4.815554
257.684102	8000.151561	13.154752	-0.053641	4.815551
257.788511	8000.141541	13.159757	-0.053661	4.815548
257.785868	8000.162880	13.164762	-0.053661	4.815554
257.719341	8000.120148	13.169767	-0.053648	4.815542
257.880350	8000.106782	13.174771	-0.053679	4.815537
257.925209	8000.111809	13.179776	-0.053687	4.815538
257.789901	8000.117087	13.184781	-0.053662	4.815541
257.934787	8000.159005	13.189786	-0.053689	4.815552
258.078364	8000.118648	13.194791	-0.053716	4.815540
257.988601	8000.150310	13.199795	-0.053700	4.815549
257.841262	8000.150049	13.204800	-0.053673	4.815550
257.930105	8000.140842	13.209805	-0.053689	4.815547
258.364721	8000.189648	13.214810	-0.053771	4.815559
258.144273	8000.141186	13.219815	-0.053730	4.815546
258.204020	8000.151798	13.224819	-0.053741	4.815549
258.203076	8000.136846	13.229824	-0.053741	4.815544
258.040501	8000.140608	13.234829	-0.053711	4.815546
257.923565	8000.159006	13.239834	-0.053689	4.815552
257.857080	8000.134433	13.244839	-0.053677	4.815545
257.883219	8000.165859	13.249843	-0.053682	4.815554
257.870142	8000.144298	13.254848	-0.053680	4.815548
257.873562	8000.140100	13.259853	-0.053681	4.815547
258.077870	8000.180856	13.264858	-0.053719	4.815558
258.016849	8000.144623	13.269863	-0.053708	4.815547
258.097021	8000.172661	13.274867	-0.053723	4.815555
258.150817	8000.176767	13.279872	-0.053733	4.815556
257.972715	8000.133272	13.284877	-0.053700	4.815544
257.984222	8000.168731	13.289882	-0.053703	4.815555
257.942463	8000.123199	13.294887	-0.053695	4.815542
258.094355	8000.147073	13.299891	-0.053724	4.815548
257.920800	8000.144246	13.304896	-0.053692	4.815548
258.017181	8000.129821	13.309901	-0.053710	4.815543
258.062070	8000.148735	13.314906	-0.053718	4.815548
258.125952	8000.115618	13.319911	-0.053730	4.815538
257.879105	8000.131886	13.324915	-0.053685	4.815544
258.024040	8000.107575	13.329920	-0.053712	4.815537
257.901606	8000.072471	13.334925	-0.053689	4.815527
257.907443	8000.118519	13.339930	-0.053691	4.815540
258.243607	8000.129390	13.344935	-0.053753	4.815542
258.283141	8000.151421	13.349939	-0.053761	4.815548
258.052391	8000.134837	13.354944	-0.053718	4.815544
258.261381	8000.117986	13.359949	-0.053757	4.815538
258.288688	8000.167591	13.364954	-0.053763	4.815553
258.027673	8000.122737	13.369959	-0.053714	4.815541
258.075215	8000.154514	13.374963	-0.053723	4.815550
258.226931	8000.153815	13.379968	-0.053752	4.815549
258.028500	8000.124943	13.384973	-0.053715	4.815542
257.982202	8000.118861	13.389978	-0.053707	4.815540
257.976224	8000.112372	13.394983	-0.053706	4.815538
258.033557	8000.124013	13.399987	-0.053717	4.815541
257.967461	8000.122948	13.404992	-0.053704	4.815541
258.224440	8000.115429	13.409997	-0.053753	4.815538
258.297094	8000.165777	13.415002	-0.053766	4.815552
258.035035	8000.112360	13.420007	-0.053718	4.815538
258.005098	8000.102274	13.425011	-0.053712	4.815535
258.216880	8000.111106	13.430016	-0.053752	4.815537
257.995590	8000.071177	13.435021	-0.053711	4.815526
258.077870	8000.148388	13.440026	-0.053727	4.815548
257.975750	8000.117890	13.445031	-0.053708	4.815540
258.115688	8000.113794	13.450035	-0.053734	4.815538
258.013755	8000.119619	13.455040	-0.053715	4.815540
258.288915	8000.097443	13.460045	-0.053767	4.815532
258.189235	8000.140692	13.465050	-0.053748	4.815545
257.951651	8000.070586	13.470055	-0.053704	4.815526
257.922044	8000.108575	13.475059	-0.053699	4.815537
257.903409	8000.162767	13.480064	-0.053696	4.815553
258.122645	8000.085195	13.485069	-0.053737	4.815529
258.156184	8000.113537	13.490074	-0.053743	4.815537
257.966877	8000.097633	13.495079	-0.053708	4.815534
258.117186	8000.132163	13.500083	-0.053736	4.815543
258.003727	8000.152754	13.505088	-0.053715	4.815550
258.103195	8000.124493	13.510093	-0.053734	4.815541
258.225986	8000.161776	13.515098	-0.053757	4.815551
258.142477	8000.135856	13.520103	-0.053742	4.815544
258.030106	8000.114804	13.525107	-0.053721	4.815538
258.244840	8000.095911	13.530112	-0.053761	4.815532
258.131238	8000.059883	13.535117	-0.053740	4.815522
258.259138	8000.104728	13.540122	-0.053764	4.815534
258.132393	8000.066349	13.545127	-0.053741	4.815524
257.925826	8000.071526	13.550131	-0.053703	4.815526
258.091206	8000.119122	13.555136	-0.053734	4.815539
258.016248	8000.142480	13.560141	-0.053720	4.815547
257.861491	8000.180554	13.565146	-0.053692	4.815558
257.809557	8000.123105	13.570151	-0.053682	4.815542
257.754127	8000.038894	13.575155	-0.053672	4.815518
258.039028	8000.130109	13.580160	-0.053725	4.815543
258.119252	8000.120761	13.585165	-0.053740	4.815540
258.106812	8000.171850	13.590170	-0.053738	4.815555
258.012449	8000.103023	13.595175	-0.053721	4.815535
258.093262	8000.120390	13.600179	-0.053736	4.815540
258.162447	8000.136498	13.605184	-0.053749	4.815544
257.921348	8000.052447	13.610189	-0.053704	4.815521
257.940026	8000.112592	13.615194	-0.053708	4.815538
257.870820	8000.109339	13.620199	-0.053696	4.815537
257.824649	8000.134238	13.625203	-0.053687	4.815545
258.120309	8000.138036	13.630208	-0.053742	4.815545
257.887860	8000.127834	13.635213	-0.053699	4.815543
257.949257	8000.160906	13.640218	-0.053711	4.815552
257.822512	8000.122527	13.645223	-0.053688	4.815542
257.896580	8000.128032	13.650227	-0.053702	4.815543
257.827933	8000.145085	13.655232	-0.053689	4.815548
257.697344	8000.126940	13.660237	-0.053665	4.815543
258.118288	8000.084721	13.665242	-0.053743	4.815529
258.131891	8000.120214	13.670247	-0.053746	4.815539
258.032525	8000.126081	13.675251	-0.053728	4.815542
258.046076	8000.131663	13.680256	-0.053731	4.815543
258.245575	8000.124270	13.685261	-0.053768	4.815540
258.164408	8000.110139	13.690266	-0.053753	4.815536
258.048654	8000.045234	13.695271	-0.053732	4.815518
258.225325	8000.070582	13.700275	-0.053765	4.815524
258.281307	8000.123861	13.705280	-0.053776	4.815540
258.051855	8000.110504	13.710285	-0.053733	4.815537
258.323489	8000.137409	13.715290	-0.053784	4.815543
258.030169	8000.085616	13.720295	-0.053729	4.815530
257.982119	8000.085915	13.725299	-0.053721	4.815530
257.794403	8000.131994	13.730304	-0.053686	4.815544
258.018815	8000.072667	13.735309	-0.053728	4.815526
258.189745	8000.121421	13.740314	-0.053760	4.815539
257.978070	8000.096605	13.745319	-0.053721	4.815533
258.115389	8000.129853	13.750323	-0.053747	4.815542
258.005642	8000.092821	13.755328	-0.053726	4.815532
257.766070	8000.066479	13.760333	-0.053682	4.815525
258.125243	8000.105501	13.765338	-0.053749	4.815535
258.316078	8000.103307	13.770343	-0.053785	4.815533
258.062911	8000.076742	13.775347	-0.053738	4.815527
258.265015	8000.073665	13.780352	-0.053776	4.815525
258.380677	8000.126855	13.785357	-0.053797	4.815540
258.196407	8000.146285	13.790362	-0.053763	4.815547
258.014345	8000.118749	13.795367	-0.053730	4.815539
258.051772	8000.136473	13.800371	-0.053737	4.815544
258.138378	8000.205210	13.805376	-0.053753	4.815564
257.841578	8000.137336	13.810381	-0.053698	4.815546
257.949949	8000.117767	13.815386	-0.053718	4.815539
257.992866	8000.101397	13.820391	-0.053727	4.815534
258.157531	8000.136163	13.825395	-0.053758	4.815544
258.166104	8000.119230	13.830400	-0.053759	4.815539
258.165036	8000.117094	13.835405	-0.053759	4.815538
258.090793	8000.138329	13.840410	-0.053746	4.815545
258.022946	8000.091301	13.845415	-0.053733	4.815531
258.078943	8000.102920	13.850419	-0.053744	4.815534
258.216950	8000.104133	13.855424	-0.053770	4.815534
258.227499	8000.061595	13.860429	-0.053772	4.815522
258.211649	8000.106219	13.865434	-0.053769	4.815535
258.291765	8000.105415	13.870439	-0.053784	4.815534
258.161147	8000.103292	13.875443	-0.053760	4.815534
258.194206	8000.058987	13.880448	-0.053767	4.815521
258.297207	8000.076717	13.885453	-0.053786	4.815526
258.358129	8000.140761	13.890458	-0.053798	4.815544
258.039436	8000.107779	13.895463	-0.053738	4.815536
257.980155	8000.105758	13.900467	-0.053728	4.815536
258.205402	8000.114810	13.905472	-0.053770	4.815537
257.902423	8000.015858	13.910477	-0.053714	4.815510
258.174592	8000.106865	13.915482	-0.053764	4.815535
258.194766	8000.046325	13.920487	-0.053768	4.815517
258.225262	8000.105596	13.925491	-0.053774	4.815534
258.295195	8000.139876	13.930496	-0.053788	4.815544
258.329688	8000.105209	13.935501	-0.053794	4.815534
258.246456	8000.104931	13.940506	-0.053779	4.815534
258.372338	8000.112355	13.945511	-0.053803	4.815536
258.258179	8000.115842	13.950515	-0.053781	4.815537
258.129828	8000.109483	13.955520	-0.053758	4.815536
258.118357	8000.100768	13.960525	-0.053756	4.815533
258.108902	8000.092085	13.965530	-0.053754	4.815531
258.218325	8000.116331	13.970535	-0.053775	4.815537
258.083107	8000.081017	13.975539	-0.053750	4.815528
257.974569	8000.125190	13.980544	-0.053730	4.815541
258.093595	8000.122887	13.985549	-0.053752	4.815540
258.195290	8000.147006	13.990554	-0.053771	4.815547
258.157450	8000.134653	13.995559	-0.053765	4.815543
257.919900	8000.159619	14.000563	-0.053721	4.815552
258.244818	8000.150010	14.005568	-0.053781	4.815547
258.165193	8000.122017	14.010573	-0.053767	4.815539
258.472998	8000.174085	14.015578	-0.053824	4.815553
258.457862	8000.134331	14.020583	-0.053822	4.815542
258.500049	8000.161747	14.025587	-0.053830	4.815549
258.457583	8000.161069	14.030592	-0.053822	4.815549
258.270301	8000.128106	14.035597	-0.053787	4.815541
258.366296	8000.156404	14.040602	-0.053805	4.815548
258.259337	8000.138645	14.045607	-0.053786	4.815544
258.098664	8000.153121	14.050611	-0.053756	4.815549
258.275416	8000.132537	14.055616	-0.053789	4.815542
258.260509	8000.177177	14.060621	-0.053787	4.815555
258.264722	8000.185810	14.065626	-0.053788	4.815557
258.199828	8000.111056	14.070631	-0.053776	4.815536
258.147733	8000.144404	14.075635	-0.053766	4.815546
258.258406	8000.133418	14.080640	-0.053787	4.815542
258.082099	8000.025860	14.085645	-0.053754	4.815512
258.402572	8000.126205	14.090650	-0.053814	4.815539
258.142800	8000.130510	14.095655	-0.053766	4.815542
258.048310	8000.120433	14.100659	-0.053749	4.815539
258.272344	8000.124125	14.105664	-0.053791	4.815539
258.129567	8000.040617	14.110669	-0.053764	4.815516
258.127365	8000.152764	14.115674	-0.053764	4.815548
258.065420	8000.111174	14.120679	-0.053753	4.815537
258.334861	8000.120951	14.125683	-0.053803	4.815538
258.307301	8000.142951	14.130688	-0.053798	4.815545
258.314444	8000.115312	14.135693	-0.053800	4.815537
258.579278	8000.176291	14.140698	-0.053849	4.815553
258.284806	8000.124478	14.145703	-0.053795	4.815539
258.334567	8000.068696	14.150707	-0.053804	4.815523
258.333301	8000.130651	14.155712	-0.053804	4.815541
258.268066	8000.130668	14.160717	-0.053792	4.815541
258.187675	8000.127232	14.165722	-0.053777	4.815541
258.029665	8000.084067	14.170727	-0.053748	4.815529
258.312193	8000.082308	14.175731	-0.053801	4.815527
258.303447	8000.118503	14.180736	-0.053800	4.815537
258.297663	8000.101335	14.185741	-0.053799	4.815532
258.388734	8000.144508	14.190746	-0.053816	4.815545
258.409507	8000.152345	14.195751	-0.053820	4.815547
258.250716	8000.152964	14.200755	-0.053791	4.815548
258.593844	8000.172497	14.205760	-0.053855	4.815552
258.345613	8000.112896	14.210765	-0.053809	4.815536
258.283444	8000.180262	14.215770	-0.053797	4.815556
258.105850	8000.148526	14.220775	-0.053764	4.815547
258.352470	8000.069266	14.225779	-0.053811	4.815523
258.369991	8000.137939	14.230784	-0.053814	4.815543
258.333771	8000.111726	14.235789	-0.053808	4.815535
258.426402	8000.135697	14.240794	-0.053825	4.815542
258.394837	8000.089263	14.245799	-0.053819	4.815528
258.284039	7999.139969	14.250803	-0.053798	4.815252

258.427090	7996.023551	14.255808	-0.053823	4.814340
258.279277	7990.589298	14.260813	-0.053792	4.812752
258.116077	7983.937870	14.265818	-0.053758	4.810807
258.121961	7976.597430	14.270823	-0.053754	4.808659
258.275754	7969.012027	14.275827	-0.053778	4.806438
258.320097	7961.207790	14.280832	-0.053782	4.804152
258.105095	7953.345778	14.285837	-0.053737	4.801849
258.185483	7945.385612	14.290842	-0.053747	4.799515
258.115834	7937.447282	14.295847	-0.053729	4.797187
257.940824	7929.394294	14.300851	-0.053691	4.794825
258.010710	7921.418001	14.305856	-0.053699	4.792482
257.881300	7913.353482	14.310861	-0.053670	4.790114
258.053930	7905.445957	14.315866	-0.053697	4.787789
257.703051	7897.362963	14.320871	-0.053627	4.785414
257.868640	7889.408981	14.325875	-0.053653	4.783074
257.778792	7881.410842	14.330880	-0.053631	4.780720
257.937844	7873.386084	14.335885	-0.053655	4.778356
257.990523	7865.445423	14.340890	-0.053660	4.776017
258.001341	7857.399032	14.345895	-0.053657	4.773645
257.788120	7849.409882	14.350899	-0.053613	4.771290
257.735565	7841.348502	14.355904	-0.053598	4.768911
257.669567	7833.385108	14.360909	-0.053580	4.766561
257.924502	7825.346093	14.365914	-0.053623	4.764186
257.604522	7817.424529	14.370919	-0.053558	4.761846
257.711957	7809.393780	14.375923	-0.053573	4.759471
257.548170	7801.457778	14.380928	-0.053538	4.757125
257.270377	7793.384189	14.385933	-0.053481	4.754736
257.364976	7785.308400	14.390938	-0.053494	4.752345
257.235459	7777.334276	14.395943	-0.053465	4.749983
257.306832	7769.314747	14.400947	-0.053473	4.747606
257.398525	7761.313113	14.405952	-0.053485	4.745233
257.202079	7753.344014	14.410957	-0.053443	4.742869
257.180559	7745.330287	14.415962	-0.053434	4.740490
257.083947	7737.386058	14.420967	-0.053411	4.738131
256.897119	7729.318887	14.425971	-0.053372	4.735735
256.997727	7721.337396	14.430976	-0.053385	4.733362
256.890685	7713.251926	14.435981	-0.053360	4.730957
256.969836	7705.345402	14.440986	-0.053370	4.728604
257.041976	7697.286526	14.445991	-0.053378	4.726205
256.844786	7689.313157	14.450995	-0.053337	4.723830
256.778750	7681.360729	14.456000	-0.053319	4.721460
256.762818	7673.254694	14.461005	-0.053311	4.719043
256.788356	7665.411584	14.466010	-0.053311	4.716703
256.626500	7657.297922	14.471015	-0.053276	4.714282
256.596943	7649.327504	14.476019	-0.053266	4.711902
256.676041	7641.301383	14.481024	-0.053275	4.709503
256.401369	7633.287110	14.486029	-0.053219	4.707108
256.510906	7625.269408	14.491034	-0.053235	4.704710
256.457519	7617.310921	14.496039	-0.053220	4.702328
256.581971	7609.283712	14.501043	-0.053238	4.699925
256.341160	7601.347715	14.506048	-0.053188	4.697548
256.202911	7593.293620	14.511053	-0.053157	4.695134
256.428585	7585.276224	14.516058	-0.053194	4.692730
256.448206	7577.289680	14.521063	-0.053193	4.690334
256.389831	7569.289076	14.526067	-0.053177	4.687932
256.370067	7561.282431	14.531072	-0.053168	4.685528
256.245324	7553.299063	14.536077	-0.053140	4.683129
256.313027	7545.317763	14.541082	-0.053148	4.680729
256.086351	7537.325520	14.546087	-0.053100	4.678326
256.018021	7529.287451	14.551091	-0.053083	4.675907
256.041442	7521.240542	14.556096	-0.053082	4.673484
255.812929	7513.122049	14.561101	-0.053034	4.671038
255.988401	7505.166048	14.566106	-0.053062	4.668640
255.699066	7497.201764	14.571111	-0.053003	4.666239
255.743727	7489.194426	14.576115	-0.053007	4.663823
255.890927	7481.284673	14.581120	-0.053029	4.661434
255.684084	7473.194730	14.586125	-0.052985	4.658991
255.700199	7465.266875	14.591130	-0.052984	4.656595
255.540952	7457.223819	14.596135	-0.052949	4.654164
255.675652	7449.225141	14.601139	-0.052969	4.651744
255.639589	7441.226999	14.606144	-0.052957	4.649323
255.558599	7433.243231	14.611149	-0.052937	4.646905
255.909539	7425.199831	14.616154	-0.052997	4.644468
255.393424	7417.245028	14.621159	-0.052896	4.642057
255.435288	7409.213410	14.626163	-0.052899	4.639621
255.442454	7401.267187	14.631168	-0.052895	4.637209
255.296473	7393.206627	14.636173	-0.052863	4.634762
255.564830	7385.172590	14.641178	-0.052908	4.632321
255.425561	7377.192471	14.646183	-0.052877	4.629896
255.560979	7369.198432	14.651187	-0.052897	4.627465
255.483785	7361.200144	14.656192	-0.052878	4.625031
255.178981	7353.201836	14.661197	-0.052816	4.622596
255.218417	7345.197807	14.666202	-0.052819	4.620158
255.184965	7337.194899	14.671207	-0.052807	4.617719
255.331502	7329.145085	14.676211	-0.052830	4.615265
255.369696	7321.226372	14.681216	-0.052832	4.612849
255.161074	7313.113485	14.686221	-0.052788	4.610373
255.278381	7305.188865	14.691226	-0.052805	4.607952
255.104835	7297.159255	14.696231	-0.052767	4.605499
255.045619	7289.181890	14.701235	-0.052751	4.603060
255.169444	7281.161662	14.706240	-0.052770	4.600607
255.125440	7273.179528	14.711245	-0.052756	4.598164
255.109579	7265.195506	14.716250	-0.052748	4.595719
254.990612	7257.171086	14.721255	-0.052721	4.593260
254.632098	7249.091373	14.726259	-0.052649	4.590783
254.825660	7241.116838	14.731264	-0.052680	4.588337
254.771357	7233.060574	14.736269	-0.052665	4.585865
254.664315	7225.124693	14.741274	-0.052640	4.583428
254.615273	7217.129943	14.746279	-0.052626	4.580972
254.655390	7209.133168	14.751283	-0.052629	4.578514
254.929222	7201.159276	14.756288	-0.052675	4.576062
254.712785	7193.100821	14.761293	-0.052629	4.573583
254.677312	7185.114149	14.766298	-0.052618	4.571124
254.429712	7177.119373	14.771303	-0.052567	4.568661
254.457750	7169.100644	14.776307	-0.052567	4.566189
254.559359	7161.087989	14.781312	-0.052581	4.563719
254.535072	7153.161087	14.786317	-0.052571	4.561273
254.585260	7145.161294	14.791322	-0.052576	4.558803
254.261946	7137.196807	14.796327	-0.052511	4.556343
254.119062	7129.089468	14.801331	-0.052479	4.553837
254.251633	7121.063033	14.806336	-0.052498	4.551355
253.933921	7113.047254	14.811341	-0.052434	4.548875
254.016620	7105.100414	14.816346	-0.052445	4.546415
253.969767	7097.116235	14.821351	-0.052431	4.543942
253.860488	7089.160953	14.826355	-0.052406	4.541477
253.907934	7081.143693	14.831360	-0.052410	4.538991
253.983801	7073.127625	14.836365	-0.052419	4.536504
253.973736	7065.119483	14.841370	-0.052412	4.534019
253.988963	7057.093473	14.846375	-0.052410	4.531526
254.019346	7049.048678	14.851379	-0.052410	4.529026
254.047797	7041.158915	14.856384	-0.052411	4.526573
253.681151	7033.089577	14.861389	-0.052337	4.524062
253.716919	7025.145311	14.866394	-0.052339	4.521590
253.631771	7017.076994	14.871399	-0.052318	4.519077
253.508991	7009.146711	14.876403	-0.052290	4.516605
253.659781	7001.064526	14.881408	-0.052313	4.514086
253.537903	6992.995982	14.886413	-0.052285	4.511569
253.553750	6985.024867	14.891418	-0.052283	4.509081
253.331202	6977.058151	14.896423	-0.052237	4.506592
253.439882	6969.061130	14.901427	-0.052252	4.504094
253.688683	6961.120195	14.906432	-0.052294	4.501612
253.505589	6953.041743	14.911437	-0.052254	4.499084
253.644225	6945.078649	14.916442	-0.052275	4.496592
253.608785	6937.074706	14.921447	-0.052264	4.494085
253.456871	6929.062415	14.926451	-0.052230	4.491574
253.526705	6921.033601	14.931456	-0.052238	4.489057
253.310543	6913.068819	14.936461	-0.052193	4.486558
253.071046	6905.027264	14.941466	-0.052144	4.484034
253.090946	6897.102951	14.946471	-0.052142	4.481545
253.189831	6889.030238	14.951475	-0.052156	4.479009
253.331041	6881.087690	14.956480	-0.052177	4.476512
253.123617	6873.029300	14.961485	-0.052133	4.473976
252.978971	6865.013545	14.966490	-0.052101	4.471453
253.175698	6857.010423	14.971495	-0.052133	4.468933
252.745424	6849.013984	14.976499	-0.052048	4.466412
252.836389	6841.032986	14.981504	-0.052060	4.463896
252.929890	6833.061378	14.986509	-0.052072	4.461381
253.172639	6825.023221	14.991514	-0.052112	4.458845
252.841885	6817.073652	14.996519	-0.052046	4.456333
252.827765	6808.981554	15.001523	-0.052038	4.453776
252.910164	6801.000492	15.006528	-0.052049	4.451253
252.603788	6792.964792	15.011533	-0.051986	4.448709
252.722539	6785.031808	15.016538	-0.052004	4.446198
252.805793	6777.016034	15.021543	-0.052014	4.443660
252.542026	6769.022269	15.026547	-0.051960	4.441125
252.546192	6761.042332	15.031552	-0.051956	4.438595
252.689855	6752.998134	15.036557	-0.051977	4.436043
252.555363	6744.978137	15.041562	-0.051947	4.433497
252.298820	6736.948818	15.046567	-0.051895	4.430945
252.174716	6728.940007	15.051571	-0.051867	4.428399
252.375607	6720.982158	15.056576	-0.051899	4.425869
252.128948	6712.943191	15.061581	-0.051848	4.423310
252.307950	6705.019274	15.066586	-0.051876	4.420788
252.314209	6696.995638	15.071591	-0.051873	4.418232
251.966195	6688.977191	15.076595	-0.051803	4.415675
252.284350	6681.011902	15.081600	-0.051857	4.413136
252.088943	6672.918317	15.086605	-0.051815	4.410552
252.004344	6664.962687	15.091610	-0.051795	4.408012
251.996275	6656.960630	15.096615	-0.051788	4.405455
251.841484	6648.961716	15.101619	-0.051754	4.402897
251.949197	6641.001242	15.106624	-0.051770	4.400351
251.725218	6633.002118	15.111629	-0.051723	4.397790
251.764170	6625.023776	15.116634	-0.051725	4.395235
251.620226	6616.972344	15.121639	-0.051693	4.392655
251.581751	6608.915125	15.126643	-0.051681	4.390071
251.545655	6600.963812	15.131648	-0.051669	4.387520
251.595701	6592.930058	15.136653	-0.051674	4.384942
251.801600	6584.993467	15.141658	-0.051707	4.382394
251.435150	6576.980456	15.146663	-0.051634	4.379817
251.286727	6568.958632	15.151667	-0.051601	4.377236
251.373503	6561.007110	15.156672	-0.051612	4.374679
251.608452	6552.959534	15.161677	-0.051651	4.372089
251.557400	6544.932682	15.166682	-0.051636	4.369503
251.577599	6536.982847	15.171687	-0.051635	4.366941
251.454818	6528.933004	15.176691	-0.051607	4.364344
251.140956	6521.030024	15.181696	-0.051544	4.361792
251.456640	6512.977371	15.186701	-0.051598	4.359194
251.439231	6505.001683	15.191706	-0.051589	4.356617
251.522866	6496.989126	15.196711	-0.051600	4.354027
251.263408	6488.857011	15.201715	-0.051547	4.351395
251.120839	6480.906904	15.206720	-0.051515	4.348821
250.943388	6472.885190	15.211725	-0.051477	4.346222
250.779873	6464.916219	15.216730	-0.051442	4.343638
250.693747	6456.985093	15.221735	-0.051421	4.341066
250.851585	6448.947730	15.226739	-0.051445	4.338460
250.990496	6440.980922	15.231744	-0.051466	4.335874
250.894821	6432.933552	15.236749	-0.051443	4.333260
250.891894	6424.899632	15.241754	-0.051437	4.330648
250.809341	6416.973078	15.246759	-0.051417	4.328070
250.710018	6408.912590	15.251763	-0.051394	4.325446
250.707397	6401.008244	15.256768	-0.051388	4.322872
250.559344	6392.948080	15.261773	-0.051356	4.320245
250.555467	6384.983433	15.266778	-0.051350	4.317649
250.637275	6376.931688	15.271783	-0.051360	4.315023
250.603319	6368.893229	15.276787	-0.051349	4.312399
250.665285	6360.904275	15.281792	-0.051355	4.309790
250.429732	6352.895610	15.286797	-0.051306	4.307171
250.645921	6344.893633	15.291802	-0.051342	4.304556
250.437162	6336.961904	15.296807	-0.051298	4.301959
250.157338	6328.885193	15.301811	-0.051241	4.299312
250.372644	6320.940662	15.306816	-0.051276	4.296712
250.462985	6312.868716	15.311821	-0.051288	4.294066
250.184540	6304.891681	15.316826	-0.051231	4.291447
250.320196	6296.889383	15.321831	-0.051251	4.288822
250.315998	6288.911593	15.326835	-0.051245	4.286202
250.190130	6280.942708	15.331840	-0.051217	4.283583
250.128271	6272.882210	15.336845	-0.051200	4.280932
250.123596	6264.913493	15.341850	-0.051194	4.278310
250.188689	6256.951662	15.346855	-0.051202	4.275689
249.996555	6248.873477	15.351859	-0.051161	4.273026
250.049750	6240.882990	15.356864	-0.051166	4.270393
249.887110	6232.881348	15.361869	-0.051130	4.267752
249.824856	6224.881118	15.366874	-0.051114	4.265112
249.841960	6216.902653	15.371879	-0.051112	4.262477
249.759750	6208.893075	15.376883	-0.051092	4.259829
249.742506	6200.922621	15.381888	-0.051083	4.257194
249.682136	6192.885661	15.386893	-0.051067	4.254534
249.597185	6184.873291	15.391898	-0.051046	4.251881
249.590009	6176.893012	15.396903	-0.051040	4.249237
249.262442	6168.886173	15.401907	-0.050974	4.246580
249.313470	6160.901124	15.406912	-0.050978	4.243932
249.283775	6152.902645	15.411917	-0.050968	4.241277
249.239693	6144.942494	15.416922	-0.050955	4.238633
249.224269	6136.923589	15.421927	-0.050947	4.235968
249.144911	6128.885311	15.426931	-0.050927	4.233294
249.159569	6120.886935	15.431936	-0.050925	4.230633
249.148559	6112.901844	15.436941	-0.050918	4.227974
249.148932	6104.890537	15.441946	-0.050913	4.225305
249.494774	6096.963927	15.446951	-0.050972	4.222666
249.174735	6088.902031	15.451955	-0.050908	4.219974
249.080273	6080.994787	15.456960	-0.050885	4.217334
249.247368	6072.894938	15.461965	-0.050911	4.214630
248.871745	6064.935345	15.466970	-0.050836	4.211966
248.890499	6056.904471	15.471975	-0.050835	4.209280
248.930397	6048.933097	15.476979	-0.050837	4.206613
248.936267	6040.923086	15.481984	-0.050833	4.203931
248.780199	6032.922316	15.486989	-0.050799	4.201249
248.834962	6024.940582	15.491994	-0.050804	4.198573
248.891986	6016.963850	15.496999	-0.050810	4.195898
248.754693	6008.853342	15.502003	-0.050779	4.193173
248.678633	6000.823321	15.507008	-0.050760	4.190475
248.755626	5992.814938	15.512013	-0.050769	4.187784
248.781841	5984.868067	15.517018	-0.050769	4.185111
248.582297	5976.930841	15.522023	-0.050727	4.182437
248.687521	5968.850718	15.527027	-0.050742	4.179717
248.802444	5960.948675	15.532032	-0.050758	4.177055
248.690395	5952.863879	15.537037	-0.050732	4.174328
248.553100	5944.896247	15.542042	-0.050702	4.171638
248.463056	5936.894337	15.547047	-0.050680	4.168934
248.414950	5928.849140	15.552051	-0.050666	4.166216
248.452335	5920.892165	15.557056	-0.050668	4.163526
248.153511	5912.906596	15.562061	-0.050607	4.160820
248.101639	5904.874549	15.567066	-0.050593	4.158101
248.178646	5896.899534	15.572071	-0.050602	4.155400
248.068982	5888.867109	15.577075	-0.050577	4.152675
248.539562	5880.833558	15.582080	-0.050659	4.149956
248.275104	5872.872256	15.587085	-0.050605	4.147250
248.055967	5864.874237	15.592090	-0.050559	4.144531
248.178863	5856.902485	15.597095	-0.050577	4.141823
248.139260	5848.838008	15.602099	-0.050565	4.139080
248.190872	5840.948030	15.607104	-0.050569	4.136395
247.877112	5832.881136	15.612109	-0.050506	4.133644
247.801420	5824.843172	15.617114	-0.050487	4.130904
247.838543	5816.855889	15.622119	-0.050489	4.128180
247.886176	5808.845130	15.627123	-0.050493	4.125447
247.990917	5800.873210	15.632128	-0.050507	4.122727
247.814105	5792.885885	15.637133	-0.050469	4.119995
247.717265	5784.931996	15.642138	-0.050446	4.117274
247.843127	5776.898457	15.647143	-0.050465	4.114527
247.767947	5768.834044	15.652147	-0.050445	4.111765
247.610454	5760.843787	15.657152	-0.050411	4.109026
247.628932	5752.839501	15.662157	-0.050410	4.106282
247.622026	5744.856999	15.667162	-0.050403	4.103543
247.527993	5736.886815	15.672167	-0.050381	4.100806
247.381956	5728.879490	15.677171	-0.050349	4.098053
247.529489	5720.897098	15.682176	-0.050371	4.095311
247.496667	5712.856258	15.687181	-0.050360	4.092545
247.192710	5704.870478	15.692186	-0.050298	4.089792
247.218979	5696.930671	15.697191	-0.050298	4.087057
247.243860	5688.885765	15.702195	-0.050298	4.084284
246.900795	5680.950517	15.707200	-0.050229	4.081543
247.016985	5672.911086	15.712205	-0.050246	4.078769
247.045684	5664.942940	15.717210	-0.050246	4.076018
246.956532	5656.940676	15.722215	-0.050224	4.073251
246.971216	5648.860279	15.727219	-0.050222	4.070456
247.069689	5640.919988	15.732224	-0.050235	4.067709
247.005111	5632.872745	15.737229	-0.050218	4.064922
246.760298	5624.927613	15.742234	-0.050168	4.062164
246.822928	5616.898800	15.747239	-0.050174	4.059381
246.758091	5608.955402	15.752243	-0.050157	4.056623
246.723350	5600.931711	15.757248	-0.050146	4.053836
246.630699	5592.880959	15.762253	-0.050124	4.051037
246.666843	5584.919246	15.767258	-0.050125	4.048269
246.510311	5576.938825	15.772263	-0.050091	4.045489
246.384370	5568.938467	15.777267	-0.050063	4.042701
246.631411	5560.901811	15.782272	-0.050104	4.039904
246.546691	5552.965380	15.787277	-0.050083	4.037135
246.445595	5544.925138	15.792282	-0.050059	4.034328
246.389816	5536.834068	15.797287	-0.050044	4.031502
246.374190	5528.813047	15.802291	-0.050036	4.028698
246.338127	5520.882402	15.807296	-0.050024	4.025925
245.952452	5512.890511	15.812301	-0.049947	4.023122
246.092772	5504.895474	15.817306	-0.049968	4.020324
246.051400	5496.939805	15.822311	-0.049956	4.017536
246.060791	5488.874407	15.827315	-0.049952	4.014708
246.153769	5480.887452	15.832320	-0.049965	4.011906
246.091078	5472.862356	15.837325	-0.049948	4.009087
246.002357	5464.901833	15.842330	-0.049927	4.006288
246.004932	5456.897534	15.847335	-0.049922	4.003473
245.991869	5448.907561	15.852339	-0.049915	4.000661
246.063034	5440.932675	15.857344	-0.049923	3.997854
245.936345	5432.913968	15.862349	-0.049894	3.995026
246.006601	5424.861865	15.867354	-0.049902	3.992188
246.026149	5416.888550	15.872359	-0.049901	3.989374
245.705015	5408.937521	15.877363	-0.049836	3.986561
245.659300	5400.905259	15.882368	-0.049823	3.983721
245.392282	5392.912029	15.887373	-0.049768	3.980890
245.353259	5384.928903	15.892378	-0.049756	3.978064
245.804753	5376.944234	15.897383	-0.049835	3.975244
245.530460	5368.896344	15.902387	-0.049779	3.972387
245.584127	5360.890709	15.907392	-0.049784	3.969548
245.208057	5352.946442	15.912397	-0.049709	3.966722
245.468468	5344.922181	15.917402	-0.049752	3.963876
245.259163	5336.974445	15.922407	-0.049708	3.961048
245.222675	5328.970620	15.927411	-0.049696	3.958200
245.438913	5320.991898	15.932416	-0.049732	3.955364
245.330318	5312.938239	15.937421	-0.049706	3.952493
245.224887	5304.893831	15.942426	-0.049682	3.949624
245.188982	5296.948145	15.947431	-0.049670	3.946789
245.010842	5288.928644	15.952435	-0.049632	3.943923
245.060469	5280.954466	15.957440	-0.049636	3.941075
244.874741	5272.954939	15.962445	-0.049597	3.938212
245.039679	5264.947340	15.967450	-0.049622	3.935350
245.123865	5256.972204	15.972455	-0.049633	3.932496
244.862042	5248.924380	15.977459	-0.049579	3.929608
245.103242	5240.969528	15.982464	-0.049619	3.926760
244.806891	5232.973607	15.987469	-0.049559	3.923885
244.812412	5224.996164	15.992474	-0.049555	3.921021
244.763551	5216.994323	15.997479	-0.049541	3.918145
244.547852	5208.972207	16.002483	-0.049496	3.915256
244.543201	5200.981694	16.007488	-0.049490	3.912380
244.626237	5192.908490	16.012493	-0.049500	3.909474
244.951022	5184.935260	16.017498	-0.049556	3.906607
244.920555	5176.955050	16.022503	-0.049545	3.903728
244.751617	5168.963754	16.027507	-0.049509	3.900840
244.507817	5160.998785	16.032512	-0.049458	3.897959
244.468441	5152.989368	16.037517	-0.049446	3.895063
244.451296	5144.983034	16.042522	-0.049438	3.892166
244.687953	5136.978732	16.047527	-0.049477	3.889273
244.531769	5128.981333	16.052531	-0.049443	3.886373
244.506538	5120.987305	16.057536	-0.049433	3.883474
244.248334	5113.013440	16.062541	-0.049380	3.880576
244.412779	5104.989446	16.067546	-0.049406	3.877665
244.502571	5096.977151	16.072551	-0.049417	3.874756
244.243979	5088.732221	16.077555	-0.049364	3.871752
244.212050	5080.803078	16.082560	-0.049353	3.868866
244.262336	5072.842833	16.087565	-0.049357	3.865968
244.216848	5064.917751	16.092570	-0.049344	3.863078
244.068108	5056.964072	16.097575	-0.049311	3.860174
244.123155	5048.930854	16.102579	-0.049317	3.857243
244.352685	5040.949620	16.107584	-0.049354	3.854332
243.964211	5032.986372	16.112589	-0.049277	3.851413
243.666629	5024.945806	16.117594	-0.049217	3.848465
243.854825	5016.977333	16.122599	-0.049247	3.845551
243.836753	5008.981235	16.127603	-0.049238	3.842621
243.898976	5001.008866	16.132608	-0.049245	3.839699
243.807274	4993.061429	16.137613	-0.049223	3.836781
243.596655	4985.032489	16.142618	-0.049179	3.833827
243.527591	4977.009439	16.147623	-0.049161	3.830877
243.717325	4968.998228	16.152627	-0.049191	3.827934
243.658878	4961.018306	16.157632	-0.049175	3.824996
243.482884	4953.044513	16.162637	-0.049137	3.822054
243.658473	4945.017772	16.167642	-0.049165	3.819099
243.460124	4937.113494	16.172647	-0.049123	3.816178
243.363713	4929.037042	16.177651	-0.049100	3.813194
243.359844	4921.032519	16.182656	-0.049094	3.810236
243.292730	4913.043815	16.187661	-0.049077	3.807280
243.200641	4905.034987	16.192666	-0.049055	3.804314
243.210102	4897.129277	16.197671	-0.049052	3.801385
243.076517	4889.067186	16.202675	-0.049022	3.798394
243.077736	4881.098601	16.207680	-0.049017	3.795438
243.186381	4873.044126	16.212685	-0.049032	3.792450
242.849579	4865.040928	16.217690	-0.048964	3.789468
243.068333	4857.039564	16.222695	-0.049000	3.786498
242.943866	4849.037264	16.227699	-0.048972	3.783517
243.044804	4841.073878	16.232704	-0.048986	3.780553
242.902637	4833.098693	16.237709	-0.048954	3.777577
242.841188	4825.085663	16.242714	-0.048938	3.774587
242.708713	4817.073292	16.247719	-0.048908	3.771592
242.869501	4809.038651	16.252723	-0.048933	3.768594
243.000223	4801.053904	16.257728	-0.048952	3.765611
242.725393	4793.106929	16.262733	-0.048896	3.762631
242.514983	4785.078262	16.267738	-0.048852	3.759619
242.569705	4777.153024	16.272743	-0.048857	3.756650
242.456303	4769.088024	16.277747	-0.048831	3.753622
242.414331	4761.041784	16.282752	-0.048818	3.750600
242.514814	4753.066285	16.287757	-0.048832	3.747606
242.474904	4745.036997	16.292762	-0.048820	3.744586
242.540736	4737.118712	16.297767	-0.048827	3.741607
242.482008	4729.106812	16.302771	-0.048811	3.738588
242.472279	4721.114888	16.307776	-0.048804	3.735576
242.459208	4713.112261	16.312781	-0.048797	3.732556
242.346547	4705.090193	16.317786	-0.048771	3.729525
242.327075	4697.127419	16.322791	-0.048762	3.726515
242.175795	4689.098621	16.327795	-0.048729	3.723476
242.360255	4681.172076	16.332800	-0.048758	3.720480
242.183404	4673.166253	16.337805	-0.048720	3.717443
242.116829	4665.165726	16.342810	-0.048703	3.714409
241.961966	4657.105086	16.347815	-0.048669	3.711347
241.979787	4649.063834	16.352819	-0.048667	3.708294
242.114219	4641.119353	16.357824	-0.048687	3.705278
241.882273	4633.165747	16.362829	-0.048639	3.702247
241.823090	4625.156657	16.367834	-0.048623	3.699197
241.805254	4617.212932	16.372839	-0.048615	3.696170
241.613762	4609.161088	16.377843	-0.048574	3.693095
241.730039	4601.148927	16.382848	-0.048591	3.690040
241.470345	4593.211493	16.387853	-0.048538	3.687002
241.685094	4585.134178	16.392858	-0.048572	3.683920
241.615072	4577.227654	16.397863	-0.048555	3.680894
241.404939	4569.217189	16.402867	-0.048510	3.677822
241.385014	4561.226867	16.407872	-0.048502	3.674759
241.310160	4553.203775	16.412877	-0.048483	3.671680
241.374651	4545.189468	16.417882	-0.048490	3.668606
241.475698	4537.187516	16.422887	-0.048504	3.665534
241.542815	4529.216440	16.427891	-0.048511	3.662471
241.299141	4521.222796	16.432896	-0.048461	3.659389
241.217412	4513.270368	16.437901	-0.048440	3.656324
241.390839	4505.210101	16.442906	-0.048468	3.653222
241.341275	4497.214728	16.447911	-0.048453	3.650136
241.026663	4489.226535	16.452915	-0.048390	3.647043
241.193918	4481.230705	16.457920	-0.048416	3.643958
240.939413	4473.262590	16.462925	-0.048364	3.640869
240.708443	4465.247328	16.467930	-0.048316	3.637760
240.734320	4457.284849	16.472935	-0.048315	3.634676
240.803209	4449.174029	16.477939	-0.048323	3.631533
240.837809	4441.211702	16.482944	-0.048325	3.628444
240.657386	4433.238241	16.487949	-0.048286	3.625342
240.761512	4425.262175	16.492954	-0.048301	3.622244
240.669189	4417.282643	16.497959	-0.048278	3.619136
240.576832	4409.297992	16.502963	-0.048256	3.616024
240.902061	4401.265123	16.507968	-0.048312	3.612902
240.689113	4393.258005	16.512973	-0.048267	3.609773
240.574208	4385.278138	16.517978	-0.048241	3.606654
240.425731	4377.331580	16.522983	-0.048208	3.603544
240.472750	4369.309365	16.527987	-0.048212	3.600408
240.618542	4361.367561	16.532992	-0.048234	3.597303
240.497915	4353.338596	16.537997	-0.048206	3.594154
240.477191	4345.314305	16.543002	-0.048198	3.591007
240.412206	4337.338424	16.548007	-0.048180	3.587874
240.188055	4329.313549	16.553011	-0.048134	3.584716
240.309224	4321.385858	16.558016	-0.048151	3.581602
240.273058	4313.357521	16.563021	-0.048140	3.578442
240.224336	4305.376036	16.568026	-0.048126	3.575297
240.188395	4297.403041	16.573031	-0.048114	3.572152
240.332378	4289.349538	16.578035	-0.048136	3.568979
240.224266	4281.397547	16.583040	-0.048111	3.565835
240.202036	4273.406811	16.588045	-0.048101	3.562676
240.011861	4265.397741	16.593050	-0.048061	3.559502
239.913567	4257.447408	16.598055	-0.048038	3.556351
239.733421	4249.342550	16.603059	-0.047999	3.553133
239.581597	4241.304367	16.608064	-0.047966	3.549940
239.572672	4233.367338	16.613069	-0.047959	3.546789
239.545361	4225.339026	16.618074	-0.047949	3.543597
239.525100	4217.377058	16.623079	-0.047940	3.540430
239.611594	4209.393809	16.628083	-0.047951	3.537254
239.503170	4201.403440	16.633088	-0.047926	3.534067
239.490232	4193.415450	16.638093	-0.047919	3.530880
239.660063	4185.402048	16.643098	-0.047945	3.527687
239.712872	4177.409421	16.648103	-0.047950	3.524495
239.409854	4169.462089	16.653107	-0.047889	3.521307
239.250649	4161.474455	16.658112	-0.047854	3.518105
239.313602	4153.488039	16.663117	-0.047861	3.514907
239.380862	4145.438503	16.668122	-0.047868	3.511681
239.391604	4137.451228	16.673127	-0.047865	3.508475
239.100523	4129.454182	16.678131	-0.047806	3.505253
239.263953	4121.510903	16.683136	-0.047832	3.502064
239.015878	4113.524561	16.688141	-0.047781	3.498842
238.844502	4105.518810	16.693146	-0.047744	3.495611
239.088370	4097.535346	16.698151	-0.047784	3.492400
238.800407	4089.493256	16.703155	-0.047725	3.489145
238.908373	4081.542848	16.708160	-0.047740	3.485936
238.859315	4073.575018	16.713165	-0.047726	3.482713
238.889783	4065.535851	16.718170	-0.047727	3.479460
238.870424	4057.600561	16.723175	-0.047718	3.476245
238.641457	4049.566868	16.728179	-0.047671	3.472980
238.915984	4041.513938	16.733184	-0.047717	3.469720
238.734283	4033.553919	16.738189	-0.047678	3.466480
238.655620	4025.556377	16.743194	-0.047658	3.463226
238.821617	4017.552961	16.748199	-0.047684	3.459974
238.672353	4009.606780	16.753203	-0.047652	3.456731
238.647314	4001.603050	16.758208	-0.047642	3.453467
238.604864	3993.588430	16.763213	-0.047629	3.450194
238.562513	3985.590596	16.768218	-0.047616	3.446925
238.184464	3977.650435	16.773223	-0.047541	3.443665
237.999261	3969.650488	16.778227	-0.047501	3.440384
238.042290	3961.667882	16.783232	-0.047504	3.437115
238.098688	3953.645353	16.788237	-0.047510	3.433826
238.043148	3945.620632	16.793242	-0.047494	3.430530
238.246012	3937.600714	16.798247	-0.047527	3.427242
238.108371	3929.642153	16.803251	-0.047497	3.423963
237.944293	3921.691941	16.808256	-0.047461	3.420685
237.881677	3913.720620	16.813261	-0.047444	3.417398
237.908581	3905.673954	16.818266	-0.047444	3.414079
238.224849	3897.671582	16.823271	-0.047498	3.410786
237.924743	3889.678163	16.828275	-0.047437	3.407472
237.883594	3881.711082	16.833280	-0.047425	3.404174
237.862738	3873.762106	16.838285	-0.047416	3.400882
237.924946	3865.734099	16.843290	-0.047422	3.397556
237.963550	3857.773062	16.848295	-0.047425	3.394254
237.716709	3849.636378	16.853299	-0.047374	3.390866
237.681477	3841.685272	16.858304	-0.047362	3.387560
237.584613	3833.730657	16.863309	-0.047339	3.384246
237.423533	3825.769839	16.868314	-0.047304	3.380924
237.476324	3817.804775	16.873319	-0.047309	3.377605
237.212982	3809.801870	16.878323	-0.047255	3.374255
237.486889	3801.761273	16.883328	-0.047301	3.370906
237.332503	3793.788988	16.888333	-0.047267	3.367566
237.105542	3785.803319	16.893338	-0.047220	3.364215
237.246584	3777.856705	16.898343	-0.047241	3.360890
237.321642	3769.824625	16.903347	-0.047250	3.357523
237.119021	3761.846044	16.908352	-0.047207	3.354166
236.980992	3753.833596	16.913357	-0.047177	3.350793
237.179456	3745.820931	16.918362	-0.047209	3.347429
237.034673	3737.844519	16.923367	-0.047177	3.344065
237.130141	3729.842001	16.928371	-0.047189	3.340695
237.245104	3721.876134	16.933376	-0.047206	3.337337
237.121205	3713.883688	16.938381	-0.047178	3.333956
236.975572	3705.873272	16.943386	-0.047146	3.330564
236.865768	3697.925449	16.948391	-0.047120	3.327195
236.707193	3689.907537	16.953395	-0.047086	3.323792
236.637671	3681.955547	16.958400	-0.047068	3.320417
236.648672	3673.976644	16.963405	-0.047065	3.317029
236.716602	3665.930375	16.968410	-0.047072	3.313612
236.722820	3657.925719	16.973415	-0.047069	3.310206
236.547465	3649.956424	16.978419	-0.047031	3.306806
236.676789	3641.959500	16.983424	-0.047050	3.303401
236.593071	3633.983926	16.988429	-0.047029	3.299994
236.434783	3626.026223	16.993434	-0.046995	3.296588
236.488763	3618.013291	16.998439	-0.047000	3.293163
236.573470	3609.964368	17.003443	-0.047011	3.289721
236.365046	3602.049240	17.008448	-0.046967	3.286321
236.136049	3594.054074	17.013453	-0.046919	3.282882
235.912222	3586.078556	17.018458	-0.046873	3.279448
235.950840	3578.121113	17.023463	-0.046875	3.276028
235.841151	3570.065797	17.028467	-0.046849	3.272557
235.838402	3562.055707	17.033472	-0.046844	3.269106
235.720169	3554.076186	17.038477	-0.046817	3.265660
235.817867	3546.080359	17.043482	-0.046830	3.262212
235.866899	3538.103896	17.048487	-0.046834	3.258766
235.721487	3530.127726	17.053491	-0.046802	3.255310
235.819994	3522.132631	17.058496	-0.046816	3.251851
235.723545	3514.134456	17.063501	-0.046793	3.248379
235.738393	3506.126696	17.068506	-0.046790	3.244904
235.901970	3498.171199	17.073511	-0.046816	3.241454
235.726201	3490.178086	17.078515	-0.046778	3.237970
235.739487	3482.197596	17.083520	-0.046776	3.234496
235.714540	3474.129739	17.088525	-0.046766	3.230978
235.641536	3466.117355	17.093530	-0.046747	3.227478
235.567266	3458.174530	17.098535	-0.046729	3.224005
235.328795	3450.191473	17.103539	-0.046679	3.220504
235.269563	3442.241013	17.108544	-0.046663	3.217021
235.401766	3434.244878	17.113549	-0.046683	3.213522
235.358626	3426.240496	17.118554	-0.046670	3.210008
235.330032	3418.279047	17.123559	-0.046659	3.206510
235.135538	3410.283819	17.128563	-0.046618	3.202986
235.044065	3402.316070	17.133568	-0.046596	3.199475
235.053851	3394.347491	17.138573	-0.046593	3.195964
235.088822	3386.294035	17.143578	-0.046594	3.192412
235.121027	3378.304894	17.148583	-0.046595	3.188885
235.025206	3370.314240	17.153587	-0.046573	3.185347
234.949611	3362.360883	17.158592	-0.046554	3.181824
234.818248	3354.390047	17.163597	-0.046524	3.178286
234.704279	3346.367402	17.168602	-0.046498	3.174722
234.891061	3338.406327	17.173607	-0.046528	3.171194
234.742432	3330.368526	17.178611	-0.046495	3.167614
234.868082	3322.388345	17.183616	-0.046513	3.164067
234.742330	3314.438631	17.188621	-0.046485	3.160518
234.435498	3306.465848	17.193626	-0.046423	3.156948
234.388541	3298.474144	17.198631	-0.046409	3.153377
234.194621	3290.434685	17.203635	-0.046368	3.149773
234.232162	3282.470415	17.208640	-0.046370	3.146209
234.216801	3274.463247	17.213645	-0.046362	3.142620
234.268355	3266.485096	17.218650	-0.046367	3.139043
234.397062	3258.507041	17.223655	-0.046386	3.135464
234.207634	3250.509013	17.228659	-0.046345	3.131859
234.244023	3242.514633	17.233664	-0.046347	3.128261
234.264869	3234.544815	17.238669	-0.046346	3.124670
234.212031	3226.579009	17.243674	-0.046331	3.121073
234.247723	3218.619150	17.248679	-0.046333	3.117478
234.234848	3210.590512	17.253683	-0.046326	3.113846
234.146357	3202.601523	17.258688	-0.046304	3.110224
233.965026	3194.625653	17.263693	-0.046265	3.106600
233.680581	3186.648881	17.268698	-0.046207	3.102966
233.859867	3178.666002	17.273703	-0.046236	3.099346
233.818539	3170.675432	17.278707	-0.046223	3.095709
233.566233	3162.707975	17.283712	-0.046171	3.092068
233.593298	3154.697916	17.288717	-0.046171	3.088416
233.422600	3146.707731	17.293722	-0.046134	3.084760
233.484157	3138.760932	17.298727	-0.046141	3.081130
233.494356	3130.763913	17.303731	-0.046138	3.077470
233.449461	3122.744552	17.308736	-0.046124	3.073794
233.466856	3114.682903	17.313741	-0.046123	3.070096
233.514196	3106.703304	17.318746	-0.046126	3.066433
233.651074	3098.733567	17.323751	-0.046147	3.062774
233.385811	3090.777863	17.328755	-0.046093	3.059099
233.280804	3082.837077	17.333760	-0.046068	3.055433
233.398465	3074.811337	17.338765	-0.046085	3.051734
233.212468	3066.828556	17.343770	-0.046045	3.048037
233.193088	3058.854558	17.348775	-0.046037	3.044347
233.187857	3050.887431	17.353779	-0.046031	3.040656
232.975093	3042.940031	17.358784	-0.045986	3.036960
232.927204	3034.930219	17.363789	-0.045972	3.033238
232.784278	3026.887125	17.368794	-0.045941	3.029491
232.918062	3018.933155	17.373799	-0.045961	3.025795
232.845906	3010.955424	17.378803	-0.045942	3.022074
232.738488	3002.984559	17.383808	-0.045917	3.018349
232.885720	2994.998265	17.388813	-0.045940	3.014624
232.823472	2986.989047	17.393818	-0.045923	3.010875
232.733318	2979.018752	17.398823	-0.045901	3.007137
232.776953	2971.012395	17.403827	-0.045904	3.003384
232.682331	2963.068479	17.408832	-0.045882	2.999649
232.561486	2955.124004	17.413837	-0.045854	2.995908
232.452519	2947.086854	17.418842	-0.045829	2.992120
232.505282	2939.085155	17.423847	-0.045834	2.988351
232.339677	2931.099534	17.428851	-0.045798	2.984574
232.314800	2923.146767	17.433856	-0.045788	2.980814
232.435954	2915.163416	17.438861	-0.045806	2.977043
232.264805	2907.197633	17.443866	-0.045769	2.973261
232.156912	2899.197815	17.448871	-0.045744	2.969461
232.251482	2891.204984	17.453875	-0.045757	2.965670
232.161262	2883.246107	17.458880	-0.045735	2.961880
231.946569	2875.280715	17.463885	-0.045690	2.958076
232.037635	2867.241031	17.468890	-0.045702	2.954248
232.186836	2859.238774	17.473895	-0.045724	2.950435
231.950301	2851.293729	17.478899	-0.045675	2.946625
231.894997	2843.314025	17.483904	-0.045660	2.942803
231.848997	2835.333292	17.488909	-0.045647	2.938976
231.816533	2827.355006	17.493914	-0.045636	2.935145
231.789414	2819.383974	17.498919	-0.045626	2.931314
231.698725	2811.379089	17.503923	-0.045604	2.927457
231.901908	2803.380519	17.508928	-0.045637	2.923614
231.687972	2795.445800	17.513933	-0.045592	2.919775
231.334062	2787.502757	17.518938	-0.045521	2.915920
231.631531	2779.407228	17.523943	-0.045571	2.912020
231.531571	2771.401569	17.528947	-0.045548	2.908137
231.458274	2763.420440	17.533952	-0.045529	2.904262
231.600940	2755.488455	17.538957	-0.045551	2.900418
231.465480	2747.543160	17.543962	-0.045520	2.896547
231.278201	2739.567532	17.548967	-0.045480	2.892653
231.163414	2731.561420	17.553971	-0.045454	2.888743
231.132326	2723.571593	17.558976	-0.045443	2.884840
231.428154	2715.615505	17.563981	-0.045493	2.880966
231.280962	2707.631478	17.568986	-0.045461	2.877049
231.233973	2699.656106	17.573991	-0.045447	2.873137
231.000551	2691.645144	17.578995	-0.045399	2.869191
231.086006	2683.674275	17.584000	-0.045410	2.865278
230.959022	2675.724822	17.589005	-0.045381	2.861357
230.932884	2667.728142	17.594010	-0.045371	2.857414
231.028784	2659.752134	17.599015	-0.045384	2.853482
230.758110	2651.762847	17.604019	-0.045329	2.849518
230.941835	2643.792009	17.609024	-0.045358	2.845582
230.890491	2635.826019	17.614029	-0.045343	2.841631
230.786097	2627.852022	17.619034	-0.045319	2.837667
230.793316	2619.883430	17.624039	-0.045315	2.833706
230.670598	2611.860557	17.629043	-0.045287	2.829706
230.521396	2603.896554	17.634048	-0.045255	2.825727
230.630205	2595.914972	17.639053	-0.045270	2.821749
230.548318	2587.947703	17.644058	-0.045250	2.817762
230.413856	2580.001527	17.649063	-0.045220	2.813776
230.394304	2571.971953	17.654067	-0.045211	2.809750
230.535615	2563.985716	17.659072	-0.045232	2.805749
230.464457	2556.037153	17.664077	-0.045214	2.801749
230.248811	2548.067095	17.669082	-0.045169	2.797723
230.234603	2540.105121	17.674087	-0.045161	2.793708
230.234967	2532.081240	17.679091	-0.045156	2.789657
230.182340	2524.115266	17.684096	-0.045142	2.785626
229.972730	2516.172327	17.689101	-0.045098	2.781591
229.869145	2508.184386	17.694106	-0.045073	2.777534
229.946153	2500.209219	17.699111	-0.045083	2.773488
229.725668	2492.199442	17.704115	-0.045037	2.769401
229.481652	2484.258873	17.709120	-0.044986	2.765342
229.899250	2476.272715	17.714125	-0.045059	2.761293
229.513891	2468.317824	17.719130	-0.044982	2.757206
229.839908	2460.284563	17.724135	-0.045038	2.753116
229.776783	2452.241322	17.729139	-0.045021	2.748990
229.614915	2444.296005	17.734144	-0.044986	2.744903
229.556554	2436.366158	17.739149	-0.044970	2.740825
229.472500	2428.382092	17.744154	-0.044950	2.736710
229.608120	2420.397342	17.749159	-0.044970	2.732602
229.383748	2412.428000	17.754163	-0.044923	2.728475
229.210806	2404.458087	17.759168	-0.044886	2.724343
229.155548	2396.539953	17.764173	-0.044871	2.720240
229.065280	2388.564587	17.769178	-0.044849	2.716098
229.123608	2380.559645	17.774183	-0.044855	2.711944
228.907558	2372.570403	17.779187	-0.044810	2.707774
228.900919	2364.601403	17.784192	-0.044803	2.703622
228.847584	2356.643081	17.789197	-0.044788	2.699466
228.792215	2348.681768	17.794202	-0.044773	2.695302
228.858097	2340.681819	17.799207	-0.044780	2.691119
228.973185	2332.679999	17.804211	-0.044797	2.686931
228.897654	2324.730858	17.809216	-0.044778	2.682753
228.832533	2316.786356	17.814221	-0.044761	2.678571
228.601908	2308.822247	17.819226	-0.044713	2.674361
228.612304	2300.806641	17.824231	-0.044710	2.670134
228.589677	2292.817184	17.829235	-0.044700	2.665911
228.598677	2284.855994	17.834240	-0.044697	2.661698
228.591828	2276.894619	17.839245	-0.044691	2.657478
228.346008	2268.922810	17.844250	-0.044640	2.653230
228.257072	2260.956138	17.849255	-0.044619	2.648988
228.391493	2252.969906	17.854259	-0.044639	2.644743
228.120685	2245.041507	17.859264	-0.044583	2.640496
228.146240	2237.081095	17.864269	-0.044583	2.636244
228.005360	2229.075034	17.869274	-0.044552	2.631950
227.996782	2221.106233	17.874279	-0.044545	2.627678
228.120127	2213.095745	17.879283	-0.044563	2.623385
228.202114	2205.142563	17.884288	-0.044573	2.619113
228.091246	2197.199576	17.889293	-0.044548	2.614827
227.970350	2189.209639	17.894298	-0.044520	2.610508
228.006007	2181.244978	17.899303	-0.044522	2.606205
227.894971	2173.289819	17.904307	-0.044496	2.601891
227.725684	2165.345978	17.909312	-0.044460	2.597572
228.096315	2157.268161	17.914317	-0.044524	2.593210
228.029708	2149.164403	17.919322	-0.044506	2.588796
227.626785	2141.287492	17.924327	-0.044426	2.584475
227.578834	2133.347718	17.929331	-0.044413	2.580138
227.477251	2125.401539	17.934336	-0.044389	2.575785
227.312004	2117.463479	17.939341	-0.044353	2.571425
227.370361	2109.457627	17.944346	-0.044359	2.567037
227.534535	2101.503705	17.949351	-0.044384	2.562676
227.353687	2093.561818	17.954355	-0.044346	2.558291
227.423918	2085.599300	17.959360	-0.044354	2.553904
227.263180	2077.630316	17.964365	-0.044319	2.549490
227.185182	2069.652313	17.969370	-0.044299	2.545069
227.223211	2061.705799	17.974375	-0.044302	2.540666
227.165344	2053.747342	17.979379	-0.044286	2.536242
227.056206	2045.766454	17.984384	-0.044260	2.531794
227.084469	2037.796079	17.989389	-0.044261	2.527354
226.909124	2029.853742	17.994394	-0.044223	2.522907
226.964618	2021.894796	17.999399	-0.044228	2.518460
226.899388	2013.914153	18.004403	-0.044211	2.513984
226.631800	2005.934326	18.009408	-0.044157	2.509485
226.675226	1997.972730	18.014413	-0.044160	2.505012
226.794007	1989.978781	18.019418	-0.044177	2.500517
226.775794	1982.045563	18.024423	-0.044168	2.496039
226.449623	1974.089185	18.029427	-0.044103	2.491517
226.672943	1966.085615	18.034432	-0.044139	2.487000
226.487696	1958.173090	18.039437	-0.044100	2.482497
226.263641	1950.225201	18.044442	-0.044053	2.477963
226.475355	1942.236650	18.049447	-0.044088	2.473429
226.432160	1934.240612	18.054451	-0.044075	2.468864
226.421886	1926.284553	18.059456	-0.044068	2.464316
226.467496	1918.342958	18.064461	-0.044071	2.459772
226.379364	1910.378598	18.069466	-0.044050	2.455196
226.460535	1902.403953	18.074471	-0.044060	2.450618
226.128770	1894.473720	18.079475	-0.043993	2.446027
225.964899	1886.524339	18.084480	-0.043958	2.441428
225.991005	1878.578775	18.089485	-0.043958	2.436837
225.875536	1870.557767	18.094490	-0.043931	2.432183
226.108766	1862.537303	18.099495	-0.043969	2.427547
225.880168	1854.600326	18.104499	-0.043922	2.422916
225.665805	1846.690432	18.109504	-0.043877	2.418292
225.781966	1838.726565	18.114509	-0.043894	2.413653
225.880580	1830.708509	18.119514	-0.043907	2.408973
225.663810	1822.797962	18.124519	-0.043862	2.404322
225.525598	1814.867678	18.129523	-0.043831	2.399656
225.662222	1806.895814	18.134528	-0.043852	2.394978
225.616495	1798.926740	18.139533	-0.043838	2.390279
225.456292	1790.962263	18.144538	-0.043803	2.385564
225.366773	1783.034995	18.149543	-0.043782	2.380867
225.511689	1775.051713	18.154547	-0.043804	2.376146
225.593321	1767.080092	18.159552	-0.043814	2.371418
225.477861	1759.139037	18.164557	-0.043787	2.366682
225.331549	1751.188026	18.169562	-0.043755	2.361929
225.216786	1743.264767	18.174567	-0.043729	2.357185
225.228848	1735.267199	18.179571	-0.043726	2.352398
225.023465	1727.321818	18.184576	-0.043683	2.347614
225.035330	1719.372911	18.189581	-0.043680	2.342836
224.665036	1711.455310	18.194586	-0.043606	2.338036
224.774808	1703.482756	18.199591	-0.043622	2.333232
224.900114	1695.466166	18.204595	-0.043640	2.328393
224.753979	1687.539155	18.209600	-0.043608	2.323576
224.671141	1679.619003	18.214605	-0.043587	2.318758
224.745033	1671.643467	18.219610	-0.043596	2.313910
224.914161	1663.651356	18.224615	-0.043623	2.309049
224.753619	1655.716288	18.229619	-0.043588	2.304185
224.656177	1647.791955	18.234624	-0.043565	2.299322
224.616607	1639.853113	18.239629	-0.043552	2.294446
224.566739	1631.862115	18.244634	-0.043538	2.289525
224.550755	1623.920826	18.249639	-0.043530	2.284628
224.350931	1616.011335	18.254643	-0.043488	2.279725
224.218281	1608.078976	18.259648	-0.043458	2.274802
224.337518	1600.021954	18.264653	-0.043475	2.269812
224.054994	1592.087629	18.269658	-0.043418	2.264854
224.162346	1584.148021	18.274663	-0.043433	2.259915
224.030083	1576.202567	18.279667	-0.043403	2.254941
223.958345	1568.247368	18.284672	-0.043385	2.249955
223.966607	1560.302417	18.289677	-0.043382	2.244971
223.893095	1552.375342	18.294682	-0.043363	2.239980
223.951789	1544.437845	18.299687	-0.043369	2.234983
223.636195	1536.490685	18.304691	-0.043305	2.229936
223.599416	1528.532749	18.309696	-0.043293	2.224895
223.483593	1520.620662	18.314701	-0.043267	2.219864
223.399461	1512.658619	18.319706	-0.043246	2.214794
223.582422	1504.666260	18.324711	-0.043275	2.209716
223.416619	1496.752497	18.329715	-0.043239	2.204645
223.478072	1488.812558	18.334720	-0.043246	2.199567
223.165744	1480.913098	18.339725	-0.043183	2.194468
223.213298	1472.902516	18.344730	-0.043187	2.189319
223.143399	1464.960734	18.349735	-0.043169	2.184192
223.116403	1457.021899	18.354739	-0.043159	2.179058
223.048955	1449.083696	18.359744	-0.043141	2.173909
223.055120	1441.131772	18.364749	-0.043137	2.168746
223.030077	1433.188838	18.369754	-0.043128	2.163573
223.013318	1425.274471	18.374759	-0.043120	2.158407
223.046746	1417.317768	18.379763	-0.043121	2.153206
222.876993	1409.379583	18.384768	-0.043084	2.147985
222.961732	1401.433371	18.389773	-0.043095	2.142770
223.001141	1393.481925	18.394778	-0.043098	2.137535
222.911785	1385.560374	18.399783	-0.043076	2.132294
222.652955	1377.645509	18.404787	-0.043023	2.127029
222.376471	1369.744499	18.409792	-0.042966	2.121758
222.252782	1361.834250	18.414797	-0.042938	2.116483
222.322231	1353.803037	18.419802	-0.042946	2.111132
222.335114	1345.840383	18.424807	-0.042944	2.105808
222.390988	1337.900448	18.429811	-0.042949	2.100489
222.177448	1330.002444	18.434816	-0.042904	2.095160
222.154031	1322.059145	18.439821	-0.042895	2.089804
222.036456	1314.123581	18.444826	-0.042868	2.084431
221.948920	1306.235935	18.449831	-0.042847	2.079080
222.035226	1298.283858	18.454835	-0.042858	2.073688
221.950055	1290.319240	18.459840	-0.042837	2.068256
221.895482	1282.414960	18.464845	-0.042822	2.062854
221.797782	1274.489883	18.469850	-0.042799	2.057420
221.894294	1266.540996	18.474855	-0.042812	2.051974
221.747928	1258.620188	18.479859	-0.042780	2.046509
221.527860	1250.715863	18.484864	-0.042734	2.041033
221.569771	1242.805642	18.489869	-0.042737	2.035564
221.387036	1234.841607	18.494874	-0.042698	2.030021
221.413765	1226.897472	18.499879	-0.042698	2.024498
221.272042	1218.997378	18.504883	-0.042666	2.018973
221.317769	1211.052284	18.509888	-0.042670	2.013420
221.332480	1203.128523	18.514893	-0.042668	2.007864
221.181837	1195.209491	18.519898	-0.042635	2.002279
221.200575	1187.310721	18.524903	-0.042633	1.996710
220.954754	1179.391705	18.529907	-0.042583	1.991083
220.979995	1171.446127	18.534912	-0.042582	1.985451
221.043197	1163.523091	18.539917	-0.042589	1.979822
220.974168	1155.609889	18.544922	-0.042571	1.974170
221.097274	1147.660177	18.549927	-0.042589	1.968496
220.972823	1139.758105	18.554931	-0.042561	1.962814
220.931808	1131.850032	18.559936	-0.042549	1.957119
220.755054	1123.928520	18.564941	-0.042511	1.951384
220.549755	1115.989039	18.569946	-0.042468	1.945615
220.728895	1108.063131	18.574951	-0.042496	1.939881
220.562055	1100.175934	18.579955	-0.042460	1.934121
220.371005	1092.252170	18.584960	-0.042419	1.928314
220.441746	1084.338441	18.589965	-0.042428	1.922525
220.319725	1076.438112	18.594970	-0.042400	1.916708
220.270464	1068.520799	18.599975	-0.042386	1.910868
220.197025	1060.594878	18.604979	-0.042367	1.905001
220.097481	1052.702614	18.609984	-0.042344	1.899138
220.249844	1044.777245	18.614989	-0.042367	1.893261
220.003328	1036.877002	18.619994	-0.042316	1.887339
220.096997	1028.969526	18.624999	-0.042329	1.881432
220.150469	1021.056980	18.630003	-0.042334	1.875498
219.896027	1013.153266	18.635008	-0.042282	1.869516
219.856841	1005.246889	18.640013	-0.042269	1.863537
219.644881	997.361468	18.645018	-0.042225	1.857536
219.793503	989.427187	18.650023	-0.042248	1.851519
219.567277	981.545984	18.655027	-0.042201	1.845480
219.496613	973.658302	18.660032	-0.042183	1.839434
219.490938	965.765479	18.665037	-0.042177	1.833372
219.344555	957.842115	18.670042	-0.042144	1.827249
219.428888	949.944912	18.675047	-0.042155	1.821154
219.503503	942.039569	18.680051	-0.042164	1.815030
219.341414	934.149715	18.685056	-0.042129	1.808870
219.349963	926.265035	18.690061	-0.042126	1.802713
219.183251	918.386265	18.695066	-0.042090	1.796518
219.045625	910.453384	18.700071	-0.042059	1.790263
219.048469	902.536964	18.705075	-0.042055	1.784016
219.033705	894.651551	18.710080	-0.042047	1.777770
218.794565	886.799724	18.715085	-0.041997	1.771500
218.678561	878.901779	18.720090	-0.041971	1.765187
218.822557	871.009299	18.725095	-0.041993	1.758887
218.752036	863.125659	18.730099	-0.041975	1.752546
218.598247	855.237212	18.735104	-0.041941	1.746166
218.403179	847.390890	18.740109	-0.041900	1.739793
218.333976	839.504991	18.745114	-0.041882	1.733379
218.542478	831.580998	18.750119	-0.041916	1.726947
218.374529	823.726208	18.755123	-0.041880	1.720498
218.423489	815.852614	18.760128	-0.041884	1.714038
218.201278	807.977054	18.765133	-0.041838	1.707516
218.184595	800.085768	18.770138	-0.041830	1.700984
218.136902	792.229468	18.775143	-0.041816	1.694451
218.202521	784.326880	18.780147	-0.041823	1.687869
218.077065	776.472589	18.785152	-0.041795	1.681276
218.061919	768.628720	18.790157	-0.041787	1.674681
217.773961	760.764662	18.795162	-0.041729	1.668006
217.945174	752.872964	18.800167	-0.041756	1.661343
217.792433	745.037120	18.805171	-0.041722	1.654656
217.879648	737.139744	18.810176	-0.041734	1.647923
217.850436	729.287607	18.815181	-0.041723	1.641185
217.566950	721.463596	18.820186	-0.041666	1.634408
217.659228	713.526641	18.825191	-0.041678	1.627557
217.543640	705.682209	18.830195	-0.041651	1.620729
217.165312	697.881724	18.835200	-0.041576	1.613873
217.190288	690.011787	18.840205	-0.041576	1.606984
217.258377	682.137231	18.845210	-0.041584	1.600067
217.174200	674.315241	18.850215	-0.041563	1.593145
217.080259	666.461249	18.855219	-0.041541	1.586163
216.846538	658.647964	18.860224	-0.041492	1.579166
217.170012	650.757483	18.865229	-0.041547	1.572150
216.778687	642.950230	18.870234	-0.041470	1.565073
216.706722	635.142338	18.875239	-0.041451	1.558010
216.791918	627.267682	18.880243	-0.041462	1.550877
216.613038	619.437201	18.885248	-0.041424	1.543713
216.753122	611.584621	18.890253	-0.041445	1.536542
216.533409	603.773770	18.895258	-0.041400	1.529322
216.442237	595.959178	18.900263	-0.041378	1.522084
216.207656	588.167076	18.905267	-0.041329	1.514810
216.308821	580.303615	18.910272	-0.041343	1.507486
216.461361	572.470105	18.915277	-0.041367	1.500162
216.171509	564.698140	18.920282	-0.041308	1.492792
216.017937	556.882506	18.925287	-0.041274	1.485364
216.140222	549.062658	18.930291	-0.041292	1.477939
215.859327	541.246763	18.935296	-0.041235	1.470417
216.011405	533.402928	18.940301	-0.041258	1.462897
215.853391	525.613866	18.945306	-0.041224	1.455342
215.653908	517.831625	18.950311	-0.041182	1.447748
215.461976	510.062337	18.955315	-0.041142	1.440127
215.458950	502.258754	18.960320	-0.041136	1.432463
215.829377	494.396686	18.965325	-0.041200	1.424761
215.573532	486.646677	18.970330	-0.041148	1.417025
215.308927	478.892455	18.975335	-0.041094	1.409242
215.524388	471.075851	18.980339	-0.041129	1.401432
215.385055	463.320092	18.985344	-0.041098	1.393580
215.430633	455.518199	18.990349	-0.041102	1.385668
215.329811	447.762754	18.995354	-0.041078	1.377734
215.068813	440.021806	19.000359	-0.041025	1.369741
214.902759	432.276832	19.005363	-0.040989	1.361713
214.554399	424.566986	19.010368	-0.040919	1.353642
214.589412	416.786273	19.015373	-0.040921	1.345516
214.592016	409.017019	19.020378	-0.040916	1.337346
214.442022	401.275693	19.025383	-0.040884	1.329129
214.569572	393.500856	19.030387	-0.040903	1.320875
214.309680	385.754744	19.035392	-0.040849	1.312530
214.201533	377.947551	19.040397	-0.040824	1.304092
214.183430	370.211220	19.045402	-0.040816	1.295694
214.269990	362.467335	19.050407	-0.040827	1.287251
214.066789	354.796459	19.055411	-0.040785	1.278780
214.021468	347.070702	19.060416	-0.040771	1.270220
214.235878	339.330009	19.065421	-0.040807	1.261635
213.817786	331.689013	19.070426	-0.040724	1.252983
213.511093	324.031861	19.075431	-0.040662	1.244274
213.484620	316.340451	19.080435	-0.040652	1.235518
213.628401	308.587991	19.085440	-0.040674	1.226662
213.491362	300.936469	19.090445	-0.040644	1.217804
213.164656	293.289798	19.095450	-0.040578	1.208850
213.461382	285.571173	19.100455	-0.040629	1.199868
213.447029	277.904912	19.105459	-0.040621	1.190818
212.982782	270.310883	19.110464	-0.040530	1.181693
212.950172	262.662466	19.115469	-0.040519	1.172520
212.694145	255.039365	19.120474	-0.040467	1.163259
212.743681	247.390722	19.125479	-0.040471	1.153957
212.756579	239.711850	19.130483	-0.040469	1.144533
212.648902	232.099581	19.135488	-0.040444	1.135089
212.635708	224.476515	19.140493	-0.040437	1.125572
212.271055	216.926870	19.145498	-0.040364	1.115991
212.310588	209.306870	19.150503	-0.040367	1.106325
212.017666	201.764593	19.155507	-0.040308	1.096601
211.878034	194.180425	19.160512	-0.040277	1.086769
211.936831	186.606462	19.165517	-0.040283	1.076905
211.763900	179.044907	19.170522	-0.040246	1.066914
211.618722	171.510790	19.175527	-0.040215	1.056872
211.551828	163.964192	19.180531	-0.040197	1.046734
211.597406	156.417191	19.185536	-0.040201	1.036523
211.646780	148.889716	19.190541	-0.040206	1.026238
211.292196	141.434745	19.195546	-0.040135	1.015853
211.176147	133.946590	19.200551	-0.040109	1.005372
211.106037	126.473103	19.205555	-0.040091	0.994812
210.854198	118.997314	19.210560	-0.040039	0.984090
210.797004	111.542400	19.215565	-0.040024	0.973330
210.840528	104.073198	19.220570	-0.040028	0.962454
210.541665	96.697970	19.225575	-0.039967	0.951504
210.341108	89.304795	19.230579	-0.039925	0.940425
210.281052	81.904174	19.235584	-0.039910	0.929241
210.079519	74.557833	19.240589	-0.039867	0.917965
209.900034	67.195755	19.245594	-0.039829	0.906531
209.926115	60.069545	19.250599	-0.039830	0.895379