Thu Mar 11 19:22:34 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.742672	0.100779	0.000000	0.000018	0.724596

0.870395	0.015424	0.005005	-0.000006	0.724474
0.868601	-0.093661	0.010010	-0.000006	0.724260
0.853730	-0.086483	0.015014	-0.000003	0.724270
0.765327	-0.072711	0.020019	0.000013	0.724266
0.808869	-0.081751	0.025024	0.000005	0.724264
0.793296	-0.076042	0.030029	0.000007	0.724270
0.677856	-0.058453	0.035034	0.000029	0.724265
0.764451	-0.071930	0.040038	0.000012	0.724269
0.808824	-0.079643	0.045043	0.000004	0.724270
0.613369	-0.046613	0.050048	0.000040	0.724267
0.811481	-0.078747	0.055053	0.000003	0.724273
0.711967	-0.066066	0.060058	0.000021	0.724264
0.719413	-0.065372	0.065062	0.000019	0.724268
0.557739	-0.036402	0.070067	0.000049	0.724269
0.761724	-0.074605	0.075072	0.000011	0.724266
0.741660	-0.155580	0.080077	0.000015	0.724101
0.588082	-0.204557	0.085082	0.000043	0.723952
0.772993	-0.235898	0.090086	0.000008	0.723955
0.897313	-0.258204	0.095091	-0.000015	0.723955
0.676532	-0.221778	0.100096	0.000026	0.723950
0.655149	-0.212287	0.105101	0.000030	0.723962
0.810991	-0.244867	0.110106	0.000001	0.723953
0.669547	-0.379313	0.115110	0.000027	0.723640
0.577507	-0.365847	0.120115	0.000044	0.723635
0.627226	-0.377699	0.125120	0.000034	0.723629
0.751253	-0.395254	0.130125	0.000011	0.723639
0.523963	-0.358345	0.135130	0.000053	0.723632
0.671777	-0.510939	0.140134	0.000025	0.723385
0.784447	-0.552869	0.145139	0.000004	0.723343
0.604445	-0.523142	0.150144	0.000037	0.723338
0.646469	-0.527015	0.155149	0.000029	0.723346
0.766900	-0.654707	0.160154	0.000007	0.723138
0.630338	-0.697141	0.165158	0.000032	0.723007
0.606375	-0.691455	0.170163	0.000036	0.723011
0.661320	-0.705071	0.175168	0.000026	0.723004
0.736041	-0.854408	0.180173	0.000012	0.722737
0.259919	-0.794823	0.185178	0.000100	0.722688
0.544894	-0.843549	0.190182	0.000047	0.722692
0.689776	-0.934185	0.195187	0.000020	0.722566
0.590487	-1.018824	0.200192	0.000038	0.722365
0.448654	-0.989647	0.205197	0.000064	0.722373
0.524999	-1.042372	0.210202	0.000050	0.722297
0.548614	-1.159746	0.215206	0.000045	0.722075
0.502466	-1.151582	0.220211	0.000054	0.722075
0.583197	-1.220489	0.225216	0.000038	0.721969
0.601175	-1.334862	0.230221	0.000035	0.721751
0.589001	-1.338666	0.235226	0.000037	0.721739
0.528364	-1.415417	0.240230	0.000048	0.721568
0.645373	-1.501149	0.245235	0.000026	0.721441
0.584449	-1.497699	0.250240	0.000037	0.721427
0.486152	-1.632520	0.255245	0.000055	0.721127
0.471845	-1.635067	0.260250	0.000058	0.721118
0.440334	-1.693954	0.265254	0.000064	0.720991
0.134736	-1.694025	0.270259	0.000120	0.720885
0.146609	-1.710911	0.275264	0.000118	0.720856
0.327827	-1.902286	0.280269	0.000084	0.720543
0.287989	-1.896118	0.285274	0.000091	0.720542
0.339626	-2.022687	0.290278	0.000081	0.720311
0.268322	-2.051506	0.295283	0.000095	0.720230
-1.418250	-1.829520	0.300288	0.000408	0.720076
-2.606597	-1.704440	0.305293	0.000629	0.719906
-3.150862	-1.611925	0.310298	0.000730	0.719898
-2.992235	-1.638208	0.315302	0.000700	0.719902
-3.242808	-1.704428	0.320307	0.000747	0.719684
-4.275179	-1.564424	0.325312	0.000939	0.719598
-4.128885	-1.585107	0.330317	0.000911	0.719609
-4.003125	-1.611280	0.335322	0.000888	0.719602
-3.698233	-1.737617	0.340326	0.000831	0.719460
-5.044767	-1.590451	0.345331	0.001081	0.719278
-4.800715	-1.639116	0.350336	0.001036	0.719268
-4.931347	-1.611986	0.355341	0.001060	0.719276
-5.171603	-1.571943	0.360346	0.001104	0.719271
-5.276965	-1.650308	0.365350	0.001124	0.719080
-5.806247	-1.614971	0.370355	0.001222	0.718964
-6.032291	-1.577616	0.375360	0.001264	0.718959
-5.955072	-1.586121	0.380365	0.001249	0.718970
-5.878121	-1.605103	0.385370	0.001235	0.718960
-5.926534	-1.631308	0.390374	0.001243	0.718892
-6.665027	-1.623629	0.395379	0.001381	0.718648
-6.921957	-1.581086	0.400384	0.001428	0.718642
-6.868294	-1.585953	0.405389	0.001418	0.718651
-6.850681	-1.592031	0.410394	0.001415	0.718646
-6.992671	-1.566677	0.415398	0.001441	0.718646
-6.824619	-1.622246	0.420403	0.001409	0.718596
-7.607137	-1.607579	0.425408	0.001555	0.718350
-7.448156	-1.631166	0.430413	0.001525	0.718360
-8.004182	-1.535509	0.435418	0.001628	0.718354
-7.837311	-1.564217	0.440422	0.001597	0.718356
-7.484736	-1.624775	0.445427	0.001531	0.718361
-7.953978	-1.549199	0.450432	0.001618	0.718346
-7.857261	-1.727947	0.455437	0.001600	0.718027
-8.166841	-1.678432	0.460442	0.001658	0.718017
-8.840926	-1.557515	0.465446	0.001783	0.718019
-8.582679	-1.602105	0.470451	0.001734	0.718022
-8.646319	-1.595407	0.475456	0.001746	0.718013
-8.776766	-1.568040	0.480461	0.001770	0.718022
-9.002261	-1.660414	0.485466	0.001812	0.717760
-9.601608	-1.582583	0.490470	0.001923	0.717704
-9.552102	-1.589876	0.495475	0.001914	0.717707
-9.655641	-1.574332	0.500480	0.001933	0.717702
-9.422726	-1.612753	0.505485	0.001889	0.717708
-9.534704	-1.597166	0.510490	0.001910	0.717700
-9.893081	-1.531927	0.515494	0.001976	0.717703
-10.008662	-1.659368	0.520499	0.001998	0.717411
-10.575918	-1.578356	0.525504	0.002103	0.717372
-10.771936	-1.539943	0.530509	0.002139	0.717379
-10.597844	-1.572349	0.535514	0.002107	0.717377
-10.497859	-1.589069	0.540518	0.002088	0.717379
-10.593555	-1.569828	0.545523	0.002106	0.717384
-10.849092	-1.526695	0.550528	0.002153	0.717380
-10.432322	-1.686231	0.555533	0.002075	0.717211
-11.263194	-1.604814	0.560538	0.002230	0.717080
-11.452022	-1.571391	0.565542	0.002265	0.717080
-11.185156	-1.615470	0.570547	0.002215	0.717087
-11.255523	-1.605318	0.575552	0.002228	0.717083
-11.231899	-1.607490	0.580557	0.002223	0.717088
-11.401675	-1.578329	0.585562	0.002254	0.717086
-11.868770	-1.654104	0.590566	0.002341	0.716772
-12.098295	-1.619347	0.595571	0.002384	0.716760
-12.873210	-1.486613	0.600576	0.002528	0.716750
-12.229989	-1.598168	0.605581	0.002408	0.716756
-12.251854	-1.595945	0.610586	0.002411	0.716753
-12.748547	-1.507722	0.615590	0.002504	0.716753
-12.483814	-1.553631	0.620595	0.002454	0.716756
-12.304696	-1.657040	0.625600	0.002421	0.716615
-13.383683	-1.547049	0.630605	0.002621	0.716453
-13.110521	-1.598561	0.635610	0.002570	0.716448
-13.200185	-1.584024	0.640614	0.002587	0.716445
-12.954925	-1.622919	0.645619	0.002541	0.716455
-13.419976	-1.545297	0.650624	0.002627	0.716445
-13.205537	-1.580988	0.655629	0.002587	0.716451
-13.038650	-1.676789	0.660634	0.002556	0.716320
-14.447380	-1.522045	0.665638	0.002818	0.716130
-14.118855	-1.577904	0.670643	0.002756	0.716136
-14.495741	-1.513501	0.675648	0.002826	0.716131
-14.150469	-1.571200	0.680653	0.002762	0.716139
-14.053176	-1.593905	0.685658	0.002744	0.716128
-14.430318	-1.524808	0.690662	0.002813	0.716133
-13.890189	-1.624704	0.695667	0.002713	0.716126
-14.984908	-1.555090	0.700672	0.002916	0.715878
-15.036239	-1.541708	0.705677	0.002926	0.715887
-14.948084	-1.560303	0.710682	0.002909	0.715881
-14.927318	-1.562521	0.715686	0.002905	0.715885
-15.018420	-1.543984	0.720691	0.002922	0.715890
-15.042542	-1.543523	0.725696	0.002926	0.715882
-14.919297	-1.561240	0.730701	0.002903	0.715891
-15.660764	-1.593639	0.735706	0.003041	0.715566
-16.122148	-1.518824	0.740710	0.003126	0.715551
-15.754874	-1.583598	0.745715	0.003058	0.715553
-15.985506	-1.547882	0.750720	0.003100	0.715543
-15.994285	-1.542870	0.755725	0.003102	0.715550
-15.877198	-1.566617	0.760730	0.003080	0.715545
-15.970029	-1.551946	0.765734	0.003097	0.715542
-16.303843	-1.597660	0.770739	0.003159	0.715333
-17.221947	-1.486846	0.775744	0.003329	0.715229
-16.719905	-1.571263	0.780749	0.003236	0.715240
-16.704507	-1.577249	0.785754	0.003233	0.715234
-17.147905	-1.498707	0.790758	0.003315	0.715233
-16.659562	-1.583241	0.795763	0.003224	0.715238
-17.119431	-1.506762	0.800768	0.003309	0.715228
-17.431829	-1.468162	0.805773	0.003367	0.715195
-17.521689	-1.594919	0.810778	0.003384	0.714912
-17.445491	-1.610161	0.815782	0.003369	0.714909
-17.870718	-1.532299	0.820787	0.003448	0.714914
-17.778744	-1.553576	0.825792	0.003431	0.714904
-17.692017	-1.564560	0.830797	0.003415	0.714914
-17.849767	-1.538753	0.835802	0.003444	0.714909
-17.882192	-1.540543	0.840806	0.003450	0.714895
-18.079989	-1.646673	0.845811	0.003486	0.714615
-18.921524	-1.499635	0.850816	0.003643	0.714609
-18.879691	-1.504116	0.855821	0.003635	0.714616
-18.323772	-1.606513	0.860826	0.003531	0.714609
-18.810364	-1.518661	0.865830	0.003621	0.714612
-18.839644	-1.511574	0.870835	0.003627	0.714616
-18.757344	-1.529869	0.875840	0.003611	0.714609
-18.860707	-1.647025	0.880845	0.003630	0.714341
-19.662703	-1.533275	0.885850	0.003779	0.714283
-19.817605	-1.507305	0.890854	0.003808	0.714280
-19.250414	-1.605071	0.895859	0.003702	0.714287
-19.633547	-1.542212	0.900864	0.003773	0.714277
-19.723146	-1.523396	0.905869	0.003789	0.714283
-19.459739	-1.573209	0.910874	0.003740	0.714278
-20.047298	-1.585025	0.915878	0.003849	0.714047
-20.505200	-1.540144	0.920883	0.003934	0.713974
-20.568437	-1.534627	0.925888	0.003946	0.713963
-20.136716	-1.604727	0.930893	0.003865	0.713977
-20.305067	-1.578755	0.935898	0.003897	0.713970
-20.706264	-1.507410	0.940902	0.003971	0.713970
-20.304144	-1.575613	0.945907	0.003896	0.713977
-20.790705	-1.593238	0.950912	0.003986	0.713770
-21.876131	-1.456047	0.955917	0.004188	0.713659
-21.306007	-1.560035	0.960922	0.004082	0.713655
-21.499862	-1.526573	0.965926	0.004118	0.713653
-21.479192	-1.527760	0.970931	0.004114	0.713658
-21.580035	-1.514480	0.975936	0.004132	0.713649
-21.255319	-1.569328	0.980941	0.004071	0.713656
-21.304786	-1.581218	0.985946	0.004080	0.713615
-22.373471	-1.520181	0.990950	0.004279	0.713358
-21.810002	-1.616392	0.995955	0.004174	0.713367
-22.430712	-1.510329	1.000960	0.004289	0.713358
-22.297053	-1.531687	1.005965	0.004264	0.713364
-22.263073	-1.538778	1.010970	0.004258	0.713362
-22.372144	-1.521206	1.015974	0.004278	0.713359
-22.246912	-1.546948	1.020979	0.004254	0.713352
-23.168361	-1.548763	1.025984	0.004426	0.713022
-23.217531	-1.536410	1.030989	0.004435	0.713030
-23.453169	-1.497226	1.035994	0.004478	0.713025
-23.407978	-1.506864	1.040998	0.004470	0.713022
-22.990866	-1.577708	1.046003	0.004392	0.713029
-23.335571	-1.521053	1.051008	0.004456	0.713020
-23.343868	-1.517120	1.056013	0.004457	0.713026
-23.319891	-1.596623	1.061018	0.004452	0.712876
-24.623355	-1.450290	1.066022	0.004695	0.712706
-24.060913	-1.545269	1.071027	0.004590	0.712717
-24.280262	-1.511847	1.076032	0.004630	0.712706
-24.203462	-1.521549	1.081037	0.004616	0.712714
-24.022884	-1.556367	1.086042	0.004582	0.712709
-24.623605	-1.450799	1.091046	0.004694	0.712707
-24.312495	-1.502328	1.096051	0.004636	0.712715
-24.776393	-1.570696	1.101056	0.004722	0.712415
-25.490086	-1.454516	1.106061	0.004854	0.712393
-25.412002	-1.470875	1.111066	0.004840	0.712389
-24.926509	-1.558770	1.116070	0.004749	0.712386
-25.309328	-1.487244	1.121075	0.004820	0.712393
-25.513562	-1.456316	1.126080	0.004858	0.712383
-25.016491	-1.540945	1.131085	0.004765	0.712391
-25.064395	-1.573800	1.136090	0.004774	0.712309
-26.353651	-1.453574	1.141094	0.005014	0.712091
-25.755700	-1.556809	1.146099	0.004902	0.712098
-26.169881	-1.487645	1.151104	0.004979	0.712090
-26.240656	-1.471996	1.156109	0.004992	0.712096
-26.153313	-1.489378	1.161114	0.004975	0.712093
-26.255180	-1.472575	1.166118	0.004994	0.712091
-25.734664	-1.562012	1.171123	0.004897	0.712098
-26.460468	-1.594453	1.176128	0.005032	0.711776
-26.950442	-1.513621	1.181133	0.005123	0.711763
-26.870004	-1.528754	1.186138	0.005108	0.711762
-26.931258	-1.519970	1.191142	0.005119	0.711758
-26.881781	-1.526259	1.196147	0.005110	0.711764
-26.837660	-1.538796	1.201152	0.005101	0.711755
-26.827246	-1.541216	1.206157	0.005099	0.711754
-27.748608	-1.526635	1.211162	0.005270	0.711456
-27.915849	-1.500489	1.216166	0.005301	0.711449
-27.954767	-1.488720	1.221171	0.005308	0.711459
-27.953660	-1.494764	1.226176	0.005308	0.711448
-27.733484	-1.530181	1.231181	0.005267	0.711456
-27.742954	-1.529997	1.236186	0.005268	0.711454
-27.887005	-1.507006	1.241190	0.005295	0.711449
-27.914510	-1.602705	1.246195	0.005300	0.711248
-28.841806	-1.493803	1.251200	0.005472	0.711136
-28.885253	-1.482910	1.256205	0.005480	0.711143
-28.879636	-1.485297	1.261210	0.005479	0.711141
-29.072486	-1.453490	1.266214	0.005514	0.711136
-28.461868	-1.558760	1.271219	0.005400	0.711143
-28.819046	-1.500252	1.276224	0.005467	0.711134
-29.180068	-1.485014	1.281229	0.005534	0.711036
-29.393876	-1.531189	1.286234	0.005573	0.710868
-29.359877	-1.537187	1.291238	0.005567	0.710869
-29.563093	-1.498488	1.296243	0.005604	0.710874
-29.424271	-1.527935	1.301248	0.005578	0.710865
-29.164934	-1.570453	1.306253	0.005530	0.710873
-29.477135	-1.515070	1.311258	0.005588	0.710873
-30.114148	-1.533762	1.316262	0.005706	0.710609
-30.479823	-1.504565	1.321267	0.005774	0.710538
-30.562781	-1.494370	1.326272	0.005789	0.710529
-30.376677	-1.524974	1.331277	0.005754	0.710535
-30.336294	-1.533203	1.336282	0.005747	0.710533
-30.611057	-1.485507	1.341286	0.005797	0.710531
-30.513566	-1.500904	1.346291	0.005779	0.710535
-30.386978	-1.612756	1.351296	0.005755	0.710357
-31.304263	-1.516217	1.356301	0.005926	0.710224
-31.134196	-1.549237	1.361306	0.005894	0.710219
-31.368320	-1.507805	1.366310	0.005937	0.710219
-31.155735	-1.542387	1.371315	0.005898	0.710226
-31.295752	-1.522256	1.376320	0.005923	0.710217
-31.396564	-1.501691	1.381325	0.005942	0.710222
-31.478060	-1.619095	1.386330	0.005957	0.709959
-32.151659	-1.532331	1.391334	0.006082	0.709893
-32.185731	-1.520069	1.396339	0.006088	0.709906
-32.380552	-1.490402	1.401344	0.006124	0.709896
-32.294196	-1.505810	1.406349	0.006108	0.709897
-32.399311	-1.488109	1.411354	0.006127	0.709895
-32.368697	-1.494324	1.416358	0.006121	0.709894
-32.006550	-1.647410	1.421363	0.006054	0.709717
-33.406504	-1.459864	1.426368	0.006314	0.709594
-33.076612	-1.516138	1.431373	0.006253	0.709599
-32.816919	-1.563803	1.436378	0.006204	0.709597
-33.203288	-1.497772	1.441382	0.006276	0.709592
-33.039273	-1.524679	1.446387	0.006245	0.709597
-33.075983	-1.521198	1.451392	0.006252	0.709591
-33.295254	-1.605655	1.456397	0.006292	0.709344
-34.096084	-1.502421	1.461402	0.006441	0.709266
-34.226204	-1.483226	1.466406	0.006465	0.709258
-33.910386	-1.535005	1.471411	0.006406	0.709268
-34.288649	-1.471391	1.476416	0.006476	0.709260
-34.009922	-1.519251	1.481421	0.006424	0.709264
-33.809012	-1.554685	1.486426	0.006387	0.709266
-33.964098	-1.613442	1.491430	0.006415	0.709093
-35.046962	-1.488151	1.496435	0.006617	0.708958
-34.807974	-1.536220	1.501440	0.006572	0.708947
-34.961000	-1.505183	1.506445	0.006600	0.708955
-35.129231	-1.474165	1.511450	0.006631	0.708958
-35.012674	-1.499089	1.516454	0.006609	0.708950
-34.668192	-1.555473	1.521459	0.006545	0.708961
-35.212116	-1.512539	1.526464	0.006646	0.708853
-36.165478	-1.449852	1.531469	0.006823	0.708638
-35.584828	-1.554061	1.536474	0.006715	0.708637
-36.069131	-1.469982	1.541478	0.006805	0.708633
-35.990917	-1.478563	1.546483	0.006790	0.708645
-36.020134	-1.477231	1.551488	0.006795	0.708637
-35.638087	-1.544951	1.556493	0.006724	0.708638
-35.638973	-1.542123	1.561498	0.006724	0.708644
-36.521770	-1.518621	1.566502	0.006888	0.708376
-36.822435	-1.477632	1.571507	0.006944	0.708352
-36.746865	-1.495052	1.576512	0.006929	0.708344
-36.551620	-1.527766	1.581517	0.006893	0.708349
-36.458879	-1.545638	1.586522	0.006875	0.708346
-36.673855	-1.509911	1.591526	0.006915	0.708342
-36.430953	-1.548821	1.596531	0.006870	0.708351
-37.333092	-1.555955	1.601536	0.007038	0.708015
-37.393041	-1.548557	1.606541	0.007049	0.708009
-37.523248	-1.525056	1.611546	0.007073	0.708010
-37.853848	-1.470353	1.616550	0.007134	0.708002
-37.599584	-1.509851	1.621555	0.007086	0.708014
-37.357814	-1.557556	1.626560	0.007041	0.708005
-37.541793	-1.522018	1.631565	0.007075	0.708011
-38.022414	-1.580497	1.636570	0.007164	0.707722
-38.735210	-1.468213	1.641574	0.007297	0.707693
-38.409433	-1.521006	1.646579	0.007236	0.707704
-38.281473	-1.547723	1.651584	0.007212	0.707697
-38.324579	-1.538891	1.656589	0.007220	0.707699
-38.301061	-1.542440	1.661594	0.007215	0.707701
-38.749475	-1.465295	1.666598	0.007298	0.707696
-38.800913	-1.587873	1.671603	0.007308	0.707432
-39.415193	-1.508348	1.676608	0.007422	0.707372
-39.576059	-1.478254	1.681613	0.007452	0.707376
-39.297338	-1.528342	1.686618	0.007400	0.707375
-39.275726	-1.533768	1.691622	0.007395	0.707372
-39.143909	-1.553743	1.696627	0.007371	0.707380
-39.802213	-1.437666	1.701632	0.007493	0.707378
-39.950005	-1.500433	1.706637	0.007520	0.707199
-40.382278	-1.480824	1.711642	0.007600	0.707084
-40.560165	-1.453022	1.716646	0.007633	0.707077
-40.307415	-1.492184	1.721651	0.007586	0.707089
-40.258209	-1.506338	1.726656	0.007577	0.707079
-40.415324	-1.474774	1.731661	0.007606	0.707087
-40.384651	-1.480338	1.736666	0.007600	0.707087
-40.344636	-1.505060	1.741670	0.007592	0.707052
-40.603885	-1.605510	1.746675	0.007640	0.706758
-41.344380	-1.478817	1.751680	0.007778	0.706748
-41.312412	-1.481736	1.756685	0.007772	0.706754
-40.796464	-1.571548	1.761690	0.007675	0.706758
-41.354718	-1.477302	1.766694	0.007779	0.706748
-41.180022	-1.506245	1.771699	0.007746	0.706753
-40.887941	-1.596134	1.776704	0.007692	0.706677
-41.877767	-1.536600	1.781709	0.007876	0.706443
-41.958129	-1.521323	1.786714	0.007891	0.706445
-42.160842	-1.488041	1.791718	0.007928	0.706440
-41.745707	-1.559342	1.796723	0.007851	0.706446
-42.390411	-1.447544	1.801728	0.007970	0.706440
-42.290062	-1.464635	1.806733	0.007951	0.706442
-41.738641	-1.597475	1.811738	0.007849	0.706373
-42.827358	-1.528680	1.816742	0.008051	0.706122
-42.909993	-1.510669	1.821747	0.008066	0.706129
-42.895199	-1.517207	1.826752	0.008063	0.706121
-42.696951	-1.549110	1.831757	0.008026	0.706129
-42.830289	-1.525554	1.836762	0.008051	0.706129
-43.178755	-1.466405	1.841766	0.008115	0.706123
-42.559225	-1.620494	1.846771	0.008000	0.706036
-43.760960	-1.493535	1.851776	0.008223	0.705861
-43.669281	-1.511023	1.856781	0.008206	0.705859
-43.291202	-1.576072	1.861786	0.008135	0.705864
-43.775623	-1.494780	1.866790	0.008225	0.705854
-43.644236	-1.513719	1.871795	0.008201	0.705864
-43.565299	-1.532311	1.876800	0.008186	0.705855
-43.722842	-1.630147	1.881805	0.008215	0.705602
-44.643689	-1.503712	1.886810	0.008386	0.705527
-44.521819	-1.529683	1.891814	0.008363	0.705519
-44.231593	-1.576204	1.896819	0.008309	0.705529
-44.598511	-1.513839	1.901824	0.008377	0.705524
-44.542567	-1.522667	1.906829	0.008366	0.705526
-44.292222	-1.586707	1.911834	0.008320	0.705488
-45.405368	-1.526834	1.916838	0.008527	0.705209
-45.301156	-1.540662	1.921843	0.008507	0.705219
-45.445127	-1.518117	1.926848	0.008534	0.705213
-45.297170	-1.543310	1.931853	0.008506	0.705216
-45.255395	-1.549962	1.936858	0.008498	0.705218
-45.642986	-1.484684	1.941862	0.008570	0.705211
-45.146113	-1.608366	1.946867	0.008477	0.705141
-46.259116	-1.536856	1.951872	0.008684	0.704886
-46.313849	-1.525335	1.956877	0.008694	0.704890
-46.111843	-1.560514	1.961882	0.008656	0.704892
-46.394524	-1.514827	1.966886	0.008709	0.704883
-46.121254	-1.558797	1.971891	0.008657	0.704893
-46.325697	-1.525043	1.976896	0.008695	0.704888
-46.462573	-1.543243	1.981901	0.008721	0.704802
-47.089161	-1.534524	1.986906	0.008837	0.704595
-47.253035	-1.509549	1.991910	0.008867	0.704587
-47.002929	-1.550129	1.996915	0.008821	0.704596
-47.099912	-1.535774	2.001920	0.008838	0.704590

-46.966979	-1.559743	2.011917	0.008813	0.704590
-47.556378	-1.535786	2.021914	0.008922	0.704428
-48.123297	-1.519072	2.031910	0.009028	0.704259
-48.185480	-1.508644	2.041907	0.009039	0.704258
-48.197571	-1.504316	2.051904	0.009041	0.704263
-47.647386	-1.510094	2.061901	0.008938	0.704450
-47.297991	-1.502465	2.071898	0.008872	0.704592
-47.036844	-1.549021	2.081894	0.008823	0.704593
-47.396332	-1.486132	2.091891	0.008890	0.704591
-47.310971	-1.502512	2.101888	0.008873	0.704590
-47.061436	-1.547890	2.111885	0.008826	0.704589
-47.209983	-1.520746	2.121882	0.008854	0.704591
-47.043618	-1.550365	2.131878	0.008822	0.704592
-47.215787	-1.520405	2.141875	0.008854	0.704591
-47.087529	-1.496107	2.151872	0.008829	0.704687
-46.324595	-1.532496	2.161869	0.008687	0.704889
-46.444997	-1.509555	2.171866	0.008709	0.704893
-46.370152	-1.525069	2.181862	0.008694	0.704889
-46.689300	-1.457268	2.191859	0.008753	0.704912
-45.803224	-1.467367	2.201856	0.008588	0.705211
-45.580446	-1.507585	2.211853	0.008546	0.705211
-45.538161	-1.513840	2.221850	0.008538	0.705214
-45.495979	-1.496358	2.231846	0.008529	0.705265
-44.785586	-1.493620	2.241843	0.008397	0.705526
-44.677789	-1.515242	2.251840	0.008376	0.705522
-44.527067	-1.541293	2.261837	0.008348	0.705525
-44.711158	-1.450603	2.271834	0.008382	0.705642
-43.600407	-1.540064	2.281830	0.008174	0.705861
-43.845963	-1.497143	2.291827	0.008220	0.705861
-43.784354	-1.508239	2.301824	0.008208	0.705861
-43.376040	-1.498368	2.311821	0.008131	0.706028
-42.880692	-1.538121	2.321818	0.008039	0.706127
-43.033898	-1.510224	2.331814	0.008067	0.706129
-43.102492	-1.480657	2.341811	0.008079	0.706164
-42.243448	-1.495447	2.351808	0.007919	0.706443
-42.151598	-1.512751	2.361805	0.007901	0.706442
-42.108065	-1.519535	2.371802	0.007892	0.706445
-41.589580	-1.511839	2.381798	0.007795	0.706647
-41.327582	-1.506057	2.391795	0.007746	0.706753
-41.126196	-1.544597	2.401792	0.007708	0.706749
-41.341997	-1.486167	2.411789	0.007748	0.706790
-40.482977	-1.494823	2.421786	0.007588	0.707081
-40.143114	-1.554738	2.431782	0.007524	0.707083
-40.569726	-1.480482	2.441779	0.007603	0.707080
-39.942793	-1.496730	2.451776	0.007486	0.707273
-39.537458	-1.519950	2.461773	0.007410	0.707372
-39.555116	-1.515943	2.471770	0.007413	0.707375
-39.333214	-1.533644	2.481766	0.007371	0.707419
-38.822081	-1.488176	2.491763	0.007275	0.707694
-38.575315	-1.531883	2.501760	0.007229	0.707696
-38.803992	-1.491432	2.511757	0.007271	0.707696
-37.997009	-1.525609	2.521754	0.007120	0.707917
-37.747643	-1.524293	2.531750	0.007073	0.708009
-37.850284	-1.507515	2.541747	0.007092	0.708007
-37.646467	-1.519241	2.551744	0.007054	0.708057
-37.178239	-1.459870	2.561741	0.006966	0.708344
-36.686719	-1.546964	2.571738	0.006874	0.708346
-36.976230	-1.496452	2.581734	0.006928	0.708345
-36.278565	-1.510955	2.591731	0.006797	0.708566
-36.156184	-1.499250	2.601728	0.006774	0.708634
-36.260212	-1.479807	2.611725	0.006793	0.708637
-35.926276	-1.483718	2.621722	0.006730	0.708749
-35.224975	-1.504694	2.631718	0.006599	0.708958
-35.248407	-1.499811	2.641715	0.006603	0.708960
-35.399430	-1.473710	2.651712	0.006631	0.708959
-34.512718	-1.479940	2.661709	0.006465	0.709264
-34.039169	-1.563629	2.671706	0.006377	0.709266
-34.258506	-1.524299	2.681702	0.006417	0.709268
-34.172731	-1.479201	2.691699	0.006401	0.709389
-33.487542	-1.498569	2.701696	0.006273	0.709596
-33.368517	-1.519542	2.711693	0.006250	0.709597
-33.112881	-1.565135	2.721690	0.006202	0.709598
-33.015532	-1.463799	2.731686	0.006183	0.709836
-32.715186	-1.486324	2.741683	0.006127	0.709899
-32.614269	-1.506766	2.751680	0.006108	0.709895
-32.483988	-1.451676	2.761677	0.006083	0.710052
-31.542805	-1.535604	2.771674	0.005907	0.710221
-31.875662	-1.476359	2.781670	0.005969	0.710221
-31.618531	-1.512673	2.791667	0.005921	0.710241
-31.016080	-1.474946	2.801664	0.005808	0.710532
-30.805749	-1.512579	2.811661	0.005768	0.710532
-30.730416	-1.526859	2.821658	0.005754	0.710532
-30.507040	-1.471142	2.831654	0.005712	0.710723
-29.602750	-1.557839	2.841651	0.005543	0.710873
-29.910095	-1.504472	2.851648	0.005600	0.710871
-29.680888	-1.547230	2.861645	0.005557	0.710868
-29.107079	-1.543457	2.871642	0.005449	0.711080
-29.177015	-1.500640	2.881638	0.005462	0.711142
-29.085452	-1.517734	2.891635	0.005445	0.711141
-29.038944	-1.472284	2.901632	0.005435	0.711249
-28.161346	-1.526618	2.911629	0.005272	0.711454
-28.376930	-1.487020	2.921626	0.005311	0.711457
-28.264731	-1.505166	2.931622	0.005290	0.711461
-27.507439	-1.489585	2.941619	0.005149	0.711762
-27.413943	-1.506827	2.951616	0.005131	0.711762
-27.270399	-1.531105	2.961613	0.005104	0.711765
-27.032419	-1.478832	2.971610	0.005059	0.711955
-26.480301	-1.506547	2.981606	0.004955	0.712097
-26.462042	-1.512304	2.991603	0.004952	0.712093
-26.674269	-1.451422	3.001600	0.004991	0.712139
-25.607325	-1.516871	3.011597	0.004792	0.712389
-25.658189	-1.506899	3.021594	0.004801	0.712391
-25.677329	-1.502893	3.031590	0.004804	0.712393
-25.092406	-1.481856	3.041587	0.004694	0.712644
-24.832327	-1.495024	3.051584	0.004646	0.712710
-24.708295	-1.516685	3.061581	0.004622	0.712712
-24.633084	-1.484153	3.071578	0.004608	0.712804
-23.833084	-1.513963	3.081574	0.004458	0.713030
-23.792411	-1.521360	3.091571	0.004450	0.713030
-23.975833	-1.491106	3.101568	0.004484	0.713026
-23.140793	-1.510190	3.111565	0.004328	0.713285
-23.030977	-1.490069	3.121562	0.004307	0.713365
-22.881468	-1.516464	3.131558	0.004279	0.713366
-23.133333	-1.442468	3.141555	0.004325	0.713425
-22.160795	-1.501456	3.151552	0.004144	0.713653
-22.082710	-1.514299	3.161549	0.004129	0.713656
-22.273560	-1.481860	3.171546	0.004164	0.713654
-21.470155	-1.493019	3.181542	0.004014	0.713917
-21.506935	-1.458893	3.191539	0.004020	0.713973
-21.365946	-1.484752	3.201536	0.003993	0.713972
-20.919814	-1.493477	3.211533	0.003910	0.714114
-20.264356	-1.523154	3.221530	0.003787	0.714287
-20.031172	-1.565319	3.231526	0.003744	0.714287
-20.481798	-1.486483	3.241523	0.003827	0.714285
-19.463209	-1.548876	3.251520	0.003637	0.714522
-19.360978	-1.520283	3.261517	0.003617	0.714616
-19.442122	-1.505897	3.271514	0.003632	0.714617
-19.029606	-1.578987	3.281510	0.003555	0.714619
-18.813227	-1.489383	3.291507	0.003514	0.714874
-18.690818	-1.491493	3.301504	0.003491	0.714914
-18.444872	-1.536246	3.311501	0.003445	0.714913
-18.394990	-1.473487	3.321498	0.003435	0.715056
-17.497344	-1.541650	3.331494	0.003267	0.715239
-17.673331	-1.510960	3.341491	0.003300	0.715238
-17.599214	-1.525061	3.351488	0.003285	0.715237
-16.762612	-1.529235	3.361485	0.003129	0.715525
-16.764619	-1.515074	3.371482	0.003129	0.715554
-16.361879	-1.585785	3.381478	0.003054	0.715556
-16.644822	-1.512786	3.391475	0.003106	0.715602
-15.758537	-1.528136	3.401472	0.002940	0.715885
-15.694278	-1.539297	3.411469	0.002928	0.715887
-15.691089	-1.539265	3.421466	0.002927	0.715889
-15.249133	-1.557802	3.431462	0.002844	0.716009
-14.894269	-1.557146	3.441459	0.002778	0.716136
-14.719403	-1.587655	3.451456	0.002745	0.716138
-14.936632	-1.549857	3.461453	0.002785	0.716138
-14.272904	-1.532112	3.471450	0.002661	0.716408
-14.018202	-1.554228	3.481446	0.002613	0.716455
-13.935797	-1.568779	3.491443	0.002597	0.716456
-13.832501	-1.538305	3.501440	0.002577	0.716553
-13.086020	-1.567870	3.511437	0.002438	0.716759
-12.924800	-1.596026	3.521434	0.002408	0.716761
-13.039193	-1.576863	3.531430	0.002428	0.716759
-12.373042	-1.573245	3.541427	0.002304	0.717002
-12.176724	-1.567676	3.551424	0.002267	0.717083
-12.209491	-1.558669	3.561421	0.002273	0.717090
-12.025633	-1.574421	3.571418	0.002238	0.717125
-11.488010	-1.538988	3.581414	0.002137	0.717385
-11.348459	-1.564349	3.591411	0.002111	0.717385
-11.293590	-1.577036	3.601408	0.002100	0.717380
-10.747128	-1.564634	3.611405	0.001998	0.717598
-10.111517	-1.621892	3.621402	0.001879	0.717709
-10.215792	-1.604020	3.631398	0.001898	0.717709
-10.233041	-1.601728	3.641395	0.001901	0.717708
-9.570439	-1.584563	3.651392	0.001777	0.717976
-9.462603	-1.582201	3.661389	0.001757	0.718019
-9.283414	-1.612523	3.671386	0.001723	0.718023
-9.382166	-1.564661	3.681382	0.001741	0.718084
-8.711788	-1.545281	3.691379	0.001616	0.718359
-8.479771	-1.586238	3.701376	0.001572	0.718360
-8.666880	-1.553495	3.711373	0.001606	0.718360
-7.825955	-1.594720	3.721370	0.001449	0.718575
-7.699511	-1.579458	3.731366	0.001425	0.718651
-7.641261	-1.591722	3.741363	0.001414	0.718648
-7.554365	-1.595190	3.751360	0.001397	0.718672
-6.921112	-1.560279	3.761357	0.001279	0.718965
-6.632042	-1.611633	3.771354	0.001225	0.718966
-6.997242	-1.547451	3.781350	0.001292	0.718965
-6.381676	-1.554024	3.791347	0.001177	0.719169
-6.134749	-1.545087	3.801344	0.001131	0.719274
-5.927387	-1.582402	3.811341	0.001092	0.719274
-5.808794	-1.565702	3.821338	0.001069	0.719350
-4.939050	-1.592741	3.831334	0.000907	0.719603
-4.832407	-1.612515	3.841331	0.000887	0.719602
-5.087113	-1.568886	3.851328	0.000934	0.719599
-4.714949	-1.549779	3.861325	0.000864	0.719768
-4.040710	-1.604834	3.871322	0.000738	0.719897
-4.069205	-1.598558	3.881318	0.000743	0.719901
-4.071043	-1.594649	3.891315	0.000743	0.719908
-3.502491	-1.535199	3.901312	0.000636	0.720226
-3.185235	-1.592955	3.911309	0.000577	0.720224
-3.214017	-1.588016	3.921306	0.000582	0.720225
-2.831290	-1.575114	3.931302	0.000510	0.720385
-2.095197	-1.624088	3.941299	0.000372	0.720548
-2.120335	-1.620909	3.951296	0.000377	0.720546
-2.145869	-1.617739	3.961293	0.000381	0.720544
-1.896839	-1.543141	3.971290	0.000334	0.720779
-1.606153	-1.540992	3.981286	0.000280	0.720886
-1.500566	-1.561053	3.991283	0.000259	0.720884
-1.556478	-1.507863	4.001280	0.000269	0.720970
-1.207305	-1.491040	4.011277	0.000204	0.721126
-1.239293	-1.486762	4.021274	0.000209	0.721124
-1.160307	-1.412707	4.031270	0.000194	0.721298
-0.992713	-1.368641	4.041267	0.000163	0.721445
-0.972204	-1.357571	4.051264	0.000158	0.721474
-0.757711	-1.256657	4.061261	0.000118	0.721749
-0.730524	-1.259974	4.071258	0.000112	0.721752
-0.659907	-1.121211	4.081254	0.000099	0.722051
-0.618851	-1.112154	4.091251	0.000091	0.722083
-0.667080	-0.967525	4.101248	0.000099	0.722351
-0.608121	-0.941546	4.111245	0.000088	0.722424
-0.470589	-0.825746	4.121242	0.000061	0.722700
-0.481957	-0.743413	4.131238	0.000063	0.722858
-0.345086	-0.690286	4.141235	0.000037	0.723011
-0.253307	-0.547211	4.151232	0.000019	0.723325
-0.452785	-0.430399	4.161229	0.000056	0.723485
-0.261439	-0.368558	4.171226	0.000020	0.723674
-0.366689	-0.205058	4.181222	0.000039	0.723958
-0.239527	-0.100080	4.191219	0.000015	0.724209
-0.283032	0.035847	4.201216	0.000022	0.724461
-0.159540	0.141968	4.211213	-0.000001	0.724712
0.000000	0.283153	4.221210	-0.000031	0.725045

0.113216	0.886437	4.226214	-0.000053	0.726264
0.284763	2.128319	4.231219	-0.000086	0.728745
0.353975	3.984524	4.236224	-0.000100	0.732372
0.788518	6.318510	4.241229	-0.000183	0.737027
0.922579	9.230449	4.246234	-0.000210	0.742655
0.951062	12.631668	4.251238	-0.000218	0.749132
1.559789	16.386347	4.256243	-0.000334	0.756409
1.976705	20.579770	4.261248	-0.000414	0.764368
2.251571	25.205480	4.266253	-0.000469	0.772992
2.904128	30.129735	4.271258	-0.000594	0.782184
3.481994	35.416850	4.276262	-0.000705	0.791895
3.757754	41.076550	4.281267	-0.000760	0.802053
4.145503	47.014425	4.286272	-0.000837	0.812603
4.820780	53.185257	4.291277	-0.000967	0.823507
5.717433	59.608424	4.296282	-0.001138	0.834763
6.390579	66.274867	4.301286	-0.001268	0.846211
7.154602	73.174705	4.306291	-0.001415	0.857918
7.872489	80.285055	4.311296	-0.001553	0.869796
8.693874	87.554200	4.316301	-0.001711	0.881799
9.420697	95.029068	4.321306	-0.001852	0.893940
10.238015	102.622923	4.326310	-0.002009	0.906129
10.764618	110.436961	4.331315	-0.002112	0.918417
11.648624	118.289790	4.336320	-0.002282	0.930697
13.641755	126.075867	4.341325	-0.002659	0.943008
14.738905	134.162447	4.346330	-0.002869	0.955372
15.255316	142.410783	4.351334	-0.002970	0.967666
16.300527	150.666222	4.356339	-0.003171	0.979950
17.647469	158.955402	4.361344	-0.003427	0.992204
18.648694	167.349711	4.366349	-0.003619	1.004371
20.230095	175.706347	4.371354	-0.003919	1.016480
21.868276	184.108486	4.376358	-0.004230	1.028522
22.714775	192.685847	4.381363	-0.004393	1.040475
23.819986	201.242416	4.386368	-0.004605	1.052325
24.584855	209.881361	4.391373	-0.004753	1.064073
25.557846	218.525099	4.396378	-0.004940	1.075746
26.902176	227.079990	4.401382	-0.005196	1.087260
28.084191	235.701006	4.406387	-0.005422	1.098703
29.494993	244.292243	4.411392	-0.005691	1.110039
30.326906	252.972458	4.416397	-0.005852	1.121247
31.282412	261.646314	4.421402	-0.006035	1.132362
32.410683	270.272736	4.426406	-0.006251	1.143346
33.838117	278.905170	4.431411	-0.006523	1.154295
35.028908	287.517088	4.436416	-0.006750	1.165067
36.035583	296.156447	4.441421	-0.006944	1.175734
36.879246	304.810448	4.446426	-0.007107	1.186289
37.671800	313.448256	4.451430	-0.007260	1.196721
38.492204	322.067321	4.456435	-0.007419	1.207046
39.912340	330.580497	4.461440	-0.007689	1.217279
40.778459	339.181932	4.466445	-0.007856	1.227419
41.690826	347.785826	4.471450	-0.008032	1.237487
42.752796	356.294150	4.476454	-0.008235	1.247394
43.303098	364.912091	4.481459	-0.008344	1.257248
44.184241	373.427846	4.486464	-0.008513	1.266973
45.005910	381.960358	4.491469	-0.008672	1.276632
46.198766	390.410667	4.496474	-0.008900	1.286195
46.926466	398.931912	4.501478	-0.009041	1.295680
47.545168	407.451873	4.506483	-0.009162	1.305074
48.554383	416.014585	4.511488	-0.009356	1.314517
48.976944	424.512360	4.516493	-0.009440	1.323718
49.981761	432.903292	4.521498	-0.009633	1.332845
50.701848	441.318322	4.526502	-0.009773	1.341885
51.190387	449.775453	4.531507	-0.009870	1.350868
51.652717	458.215156	4.536512	-0.009962	1.359768
52.072528	466.632395	4.541517	-0.010045	1.368580
52.940016	474.995250	4.546522	-0.010213	1.377356
53.294770	483.403784	4.551526	-0.010284	1.386035
53.630416	491.839477	4.556531	-0.010353	1.394685
54.337480	500.161717	4.561536	-0.010490	1.403229
54.611255	508.551511	4.566541	-0.010547	1.411716
55.163236	516.894797	4.571546	-0.010655	1.420153
55.777142	525.210324	4.576550	-0.010775	1.428522
56.051607	533.581031	4.581555	-0.010832	1.436841
56.441963	541.905656	4.586560	-0.010910	1.445085
56.936810	550.214160	4.591565	-0.011008	1.453284
57.594217	558.501906	4.596570	-0.011136	1.461442
57.865447	566.853658	4.601574	-0.011192	1.469555
58.262916	575.191578	4.606579	-0.011272	1.477631
59.173825	583.389629	4.611584	-0.011447	1.485609
59.783338	591.665498	4.616589	-0.011566	1.493571
60.172407	599.959497	4.621594	-0.011644	1.501473
60.798513	608.204530	4.626598	-0.011766	1.509325
61.153140	616.510998	4.631603	-0.011838	1.517152
61.354862	624.796325	4.636608	-0.011881	1.524895
61.972960	633.021959	4.641613	-0.012002	1.532607
62.325085	641.296687	4.646618	-0.012073	1.540285
62.630162	649.554962	4.651622	-0.012135	1.547904
63.032252	657.822704	4.656627	-0.012216	1.555507
63.524181	666.036620	4.661632	-0.012313	1.563038
63.870164	674.266063	4.666637	-0.012383	1.570526
64.187047	682.527245	4.671642	-0.012448	1.578001
64.589975	690.723631	4.676646	-0.012528	1.585397
65.021797	698.966108	4.681651	-0.012614	1.592802
65.328695	707.183428	4.686656	-0.012677	1.600133
65.827788	715.376980	4.691661	-0.012775	1.607437
66.240166	723.618765	4.696666	-0.012858	1.614738
66.540717	731.823104	4.701670	-0.012919	1.621958
66.963112	740.045445	4.706675	-0.013004	1.629178
67.515504	748.275184	4.711680	-0.013112	1.636390
67.662604	756.479692	4.716685	-0.013145	1.643493
67.976124	764.681748	4.721690	-0.013209	1.650586
68.328943	772.860949	4.726694	-0.013280	1.657634
68.629032	781.042108	4.731699	-0.013342	1.664647
68.906154	789.252199	4.736704	-0.013399	1.671652
69.271013	797.430968	4.741709	-0.013472	1.678613
69.760648	805.583475	4.746714	-0.013569	1.685539
70.004580	813.779630	4.751718	-0.013620	1.692441
70.423376	821.948762	4.756723	-0.013703	1.699316
71.028252	830.093508	4.761728	-0.013822	1.706166
71.155373	838.328785	4.766733	-0.013851	1.713002
71.628775	846.480447	4.771738	-0.013945	1.719786
72.049932	854.614773	4.776742	-0.014028	1.726523
72.256073	862.831710	4.781747	-0.014072	1.733273
72.782550	870.963373	4.786752	-0.014176	1.739969
73.014306	879.137233	4.791757	-0.014225	1.746635
73.662347	887.286601	4.796762	-0.014351	1.753309
73.790071	895.458305	4.801766	-0.014380	1.759910
74.063195	903.622399	4.806771	-0.014437	1.766498
74.521744	911.777450	4.811776	-0.014528	1.773077
74.896187	919.916303	4.816781	-0.014603	1.779609
75.278913	928.065063	4.821786	-0.014680	1.786126
75.375264	936.304237	4.826790	-0.014703	1.792655
75.809476	944.443841	4.831795	-0.014789	1.799123
75.932345	952.589481	4.836800	-0.014818	1.805535
76.078321	960.750265	4.841805	-0.014851	1.811938
76.741517	968.836189	4.846810	-0.014980	1.818323
77.102467	976.954919	4.851814	-0.015052	1.824675
77.330034	985.118604	4.856819	-0.015100	1.831024
77.672454	993.271118	4.861824	-0.015170	1.837355
78.037519	1001.379894	4.866829	-0.015243	1.843634
78.557424	1009.508643	4.871834	-0.015345	1.849924
78.620078	1017.685654	4.876838	-0.015363	1.856177
78.927212	1025.814923	4.881843	-0.015425	1.862401
79.265238	1033.954197	4.886848	-0.015494	1.868615
79.404707	1042.132792	4.891853	-0.015525	1.874815
79.929203	1050.218532	4.896858	-0.015628	1.880969
80.080789	1058.352200	4.901862	-0.015662	1.887096
80.248198	1066.502753	4.906867	-0.015699	1.893217
80.749714	1074.601076	4.911872	-0.015798	1.899318
81.163583	1082.675091	4.916877	-0.015880	1.905371
81.508942	1090.832141	4.921882	-0.015950	1.911459
81.619421	1098.975528	4.926886	-0.015976	1.917491
81.787908	1107.096881	4.931891	-0.016013	1.923494
82.216322	1115.210752	4.936896	-0.016098	1.929502
82.442476	1123.336575	4.941901	-0.016146	1.935477
82.709539	1131.465943	4.946906	-0.016201	1.941441
83.111565	1139.559045	4.951910	-0.016282	1.947375
83.502149	1147.721367	4.956915	-0.016360	1.953340
83.399182	1155.887841	4.961920	-0.016346	1.959236
83.777643	1163.928563	4.966925	-0.016422	1.965075
84.208785	1172.035898	4.971930	-0.016508	1.970951
84.226056	1180.173966	4.976934	-0.016517	1.976787
84.708194	1188.237751	4.981939	-0.016612	1.982602
84.882187	1196.374790	4.986944	-0.016650	1.988420
85.131830	1204.501703	4.991949	-0.016702	1.994221
85.454588	1212.579657	4.996954	-0.016767	1.999979
85.609447	1220.681727	5.001958	-0.016802	2.005719
86.011295	1228.775471	5.006963	-0.016882	2.011463
86.384816	1236.870851	5.011968	-0.016957	2.017188
86.408192	1245.001088	5.016973	-0.016967	2.022885
86.827782	1253.096755	5.021978	-0.017051	2.028583
87.051044	1261.236603	5.026982	-0.017098	2.034276
87.340289	1269.304676	5.031987	-0.017157	2.039909
87.795612	1277.370913	5.036992	-0.017247	2.045543
88.008668	1285.471995	5.041997	-0.017293	2.051160
88.410757	1293.577091	5.047002	-0.017373	2.056784
88.637148	1301.665106	5.052006	-0.017421	2.062363
88.899857	1309.769916	5.057011	-0.017475	2.067942
88.785856	1317.957975	5.062016	-0.017459	2.073525
89.163424	1325.997320	5.067021	-0.017535	2.079041
89.676711	1334.048471	5.072026	-0.017636	2.084564
89.700925	1342.177234	5.077030	-0.017646	2.090076
90.278681	1350.253879	5.082035	-0.017759	2.095593
90.489052	1358.349409	5.087040	-0.017804	2.101072
90.854919	1366.416091	5.092045	-0.017877	2.106532
91.257484	1374.563017	5.097050	-0.017958	2.112035
91.689992	1382.652436	5.102054	-0.018044	2.117489
91.872253	1390.734473	5.107059	-0.018083	2.122899
92.094886	1398.822081	5.112064	-0.018130	2.128303
92.367853	1406.911426	5.117069	-0.018187	2.133700
92.869120	1414.970294	5.122074	-0.018286	2.139084
92.951004	1423.070459	5.127078	-0.018306	2.144442
93.022814	1431.187897	5.132083	-0.018325	2.149797
93.380276	1439.279345	5.137088	-0.018397	2.155149
93.764016	1447.306859	5.142093	-0.018474	2.160448
93.985644	1455.399001	5.147098	-0.018521	2.165761
94.097820	1463.504735	5.152102	-0.018547	2.171059
94.456393	1471.589579	5.157107	-0.018620	2.176354
94.594595	1479.690288	5.162112	-0.018651	2.181626
94.999674	1487.736436	5.167117	-0.018732	2.186874
95.265285	1495.869142	5.172122	-0.018787	2.192153
95.653139	1503.930179	5.177126	-0.018864	2.197384
95.797082	1512.013073	5.182131	-0.018897	2.202594
96.267674	1520.056262	5.187136	-0.018990	2.207796
96.339371	1528.172006	5.192141	-0.019009	2.212996
96.797682	1536.233948	5.197146	-0.019099	2.218184
97.005474	1544.302929	5.202150	-0.019144	2.223343
97.291415	1552.386743	5.207155	-0.019202	2.228505
97.481383	1560.525391	5.212160	-0.019243	2.233682
97.715761	1568.569631	5.217165	-0.019292	2.238791
98.215349	1576.615956	5.222170	-0.019391	2.243913
98.179790	1584.724370	5.227174	-0.019390	2.249015
98.333119	1592.829616	5.232179	-0.019424	2.254120
98.559917	1600.906245	5.237184	-0.019471	2.259203
98.879971	1608.938810	5.242189	-0.019536	2.264254
99.147465	1617.032903	5.247194	-0.019592	2.269327
99.391854	1625.188423	5.252198	-0.019643	2.274426
99.576680	1633.213177	5.257203	-0.019683	2.279427
99.989593	1641.244127	5.262208	-0.019765	2.284440
100.115156	1649.308878	5.267213	-0.019794	2.289438
100.670435	1657.366642	5.272218	-0.019903	2.294458
101.048384	1665.402111	5.277222	-0.019979	2.299438
101.260921	1673.470093	5.282227	-0.020024	2.304413
101.541397	1681.575161	5.287232	-0.020081	2.309406
101.812500	1689.645104	5.292237	-0.020137	2.314365
102.178377	1697.694006	5.297242	-0.020211	2.319309
102.595942	1705.728149	5.302246	-0.020294	2.324238
102.926146	1713.815459	5.307251	-0.020361	2.329181
103.153437	1721.930844	5.312256	-0.020409	2.334123
103.321519	1729.990056	5.317261	-0.020446	2.339014
103.743942	1738.032529	5.322266	-0.020530	2.343907
104.078123	1746.110024	5.327270	-0.020598	2.348803
104.283983	1754.229247	5.332275	-0.020641	2.353703
104.621055	1762.281948	5.337280	-0.020710	2.358564
104.657992	1770.351294	5.342285	-0.020722	2.363400
104.938244	1778.417760	5.347290	-0.020780	2.368245
105.215336	1786.488532	5.352294	-0.020837	2.373081
105.594985	1794.528594	5.357299	-0.020913	2.377898
105.811480	1802.603423	5.362304	-0.020959	2.382713
106.011982	1810.655242	5.367309	-0.021001	2.387503
106.432095	1818.732560	5.372314	-0.021085	2.392316
106.602610	1826.804197	5.377318	-0.021122	2.397095
106.693354	1834.871155	5.382323	-0.021145	2.401857
106.971030	1842.943648	5.387328	-0.021202	2.406627
107.135225	1851.009372	5.392333	-0.021238	2.411374
107.246193	1859.102978	5.397338	-0.021264	2.416124
107.408431	1867.155291	5.402342	-0.021300	2.420845
107.860657	1875.181840	5.407347	-0.021390	2.425564
108.292656	1883.261340	5.412352	-0.021475	2.430303
108.494297	1891.392144	5.417357	-0.021519	2.435045
108.926255	1899.416205	5.422362	-0.021604	2.439733
109.074325	1907.440723	5.427366	-0.021637	2.444391
109.293808	1915.503985	5.432371	-0.021684	2.449067
109.767525	1923.561647	5.437376	-0.021777	2.453751
109.830222	1931.621826	5.442381	-0.021795	2.458396
110.063572	1939.667637	5.447386	-0.021844	2.463037
110.439562	1947.708791	5.452390	-0.021919	2.467677
110.557226	1955.805296	5.457395	-0.021946	2.472320
110.860327	1963.863157	5.462400	-0.022008	2.476947
110.885859	1971.901418	5.467405	-0.022019	2.481533
111.374268	1979.930713	5.472410	-0.022115	2.486140
111.486987	1988.018147	5.477414	-0.022141	2.490744
111.833993	1996.076802	5.482419	-0.022211	2.495340
112.113031	2004.130622	5.487424	-0.022269	2.499919
112.597806	2012.120310	5.492429	-0.022365	2.504469
112.819626	2020.223268	5.497434	-0.022411	2.509056
113.050049	2028.326775	5.502438	-0.022460	2.513635
113.245690	2036.382953	5.507443	-0.022502	2.518176
113.251149	2044.445054	5.512448	-0.022508	2.522699
113.492276	2052.477225	5.517453	-0.022559	2.527214
113.970700	2060.503919	5.522458	-0.022653	2.531734
114.114118	2068.592519	5.527462	-0.022685	2.536257
114.264082	2076.637595	5.532467	-0.022719	2.540749
115.875008	2084.540560	5.537472	-0.023024	2.545256
116.494631	2092.596349	5.542477	-0.023145	2.549771
116.879305	2100.693800	5.547482	-0.023222	2.554283
116.829140	2108.798750	5.552486	-0.023218	2.558762
117.197768	2116.828674	5.557491	-0.023292	2.563220
117.761247	2124.881095	5.562496	-0.023403	2.567697
117.764662	2132.977082	5.567501	-0.023409	2.572150
117.951044	2141.070050	5.572506	-0.023449	2.576607
118.252840	2149.099944	5.577510	-0.023511	2.581030
118.420870	2157.155454	5.582515	-0.023547	2.585450
118.778017	2165.228615	5.587520	-0.023619	2.589885
118.963758	2173.467068	5.592525	-0.023660	2.594390
119.391540	2181.448949	5.597530	-0.023745	2.598765
119.205812	2189.504973	5.602534	-0.023716	2.603130
119.665974	2197.476128	5.607539	-0.023807	2.607487
119.929949	2205.518461	5.612544	-0.023861	2.611861
119.880021	2213.585391	5.617549	-0.023857	2.616220
120.340202	2221.603391	5.622554	-0.023949	2.620579
120.720832	2229.606318	5.627558	-0.024025	2.624918
120.745058	2237.688539	5.632563	-0.024035	2.629268
120.969450	2245.767618	5.637568	-0.024082	2.633623
121.210808	2253.789662	5.642573	-0.024133	2.637941
121.627145	2261.804359	5.647578	-0.024215	2.642259
121.915778	2269.841381	5.652582	-0.024275	2.646574
122.277433	2277.880113	5.657587	-0.024347	2.650888
122.660461	2285.961509	5.662592	-0.024424	2.655218
123.141336	2293.953912	5.667597	-0.024519	2.659501
123.520994	2302.010084	5.672602	-0.024595	2.663803
123.757585	2310.088101	5.677606	-0.024645	2.668102
123.952120	2318.160794	5.682611	-0.024687	2.672387
124.426310	2326.214390	5.687616	-0.024780	2.676674
124.551586	2334.247083	5.692621	-0.024809	2.680920
124.929691	2342.271487	5.697626	-0.024885	2.685171
124.968746	2350.338515	5.702630	-0.024898	2.689416
125.122818	2358.396117	5.707635	-0.024932	2.693657
125.572154	2366.439895	5.712640	-0.025021	2.697903
125.695106	2374.470199	5.717645	-0.025049	2.702114
125.904458	2382.549968	5.722650	-0.025094	2.706350
126.013309	2390.593497	5.727654	-0.025120	2.710554
126.145618	2398.671366	5.732659	-0.025150	2.714771
126.220172	2406.723132	5.737664	-0.025169	2.718964
126.432610	2414.733036	5.742669	-0.025214	2.723138
126.783025	2422.772066	5.747674	-0.025285	2.727328
126.792754	2430.834604	5.752678	-0.025292	2.731504
127.075236	2438.888603	5.757683	-0.025350	2.735685
127.356891	2446.909799	5.762688	-0.025408	2.739843
127.599506	2454.935843	5.767693	-0.025459	2.743995
127.934280	2462.997303	5.772698	-0.025527	2.748164
128.329637	2471.081696	5.777702	-0.025606	2.752342
128.786200	2479.119034	5.782707	-0.025696	2.756493
129.052113	2487.146638	5.787712	-0.025751	2.760622
129.206111	2495.158013	5.792717	-0.025785	2.764729
129.410168	2503.212237	5.797722	-0.025829	2.768855
129.576462	2511.281176	5.802726	-0.025865	2.772980
129.497659	2519.338080	5.807731	-0.025856	2.777078
129.951907	2527.352104	5.812736	-0.025946	2.781180
130.233673	2535.360138	5.817741	-0.026004	2.785263
130.504103	2543.422078	5.822746	-0.026060	2.789366
130.739845	2551.506861	5.827750	-0.026109	2.793473
130.987272	2559.509000	5.832755	-0.026161	2.797533
131.271656	2567.566300	5.837760	-0.026219	2.801616
131.476459	2575.575897	5.842765	-0.026263	2.805665
131.774302	2583.631167	5.847770	-0.026323	2.809736
131.986017	2591.705712	5.852774	-0.026368	2.813807
132.174228	2599.728778	5.857779	-0.026409	2.817844
132.399893	2607.780994	5.862784	-0.026456	2.821892
132.638921	2615.817777	5.867789	-0.026506	2.825927
132.880334	2623.865290	5.872794	-0.026557	2.829962
132.981574	2631.972345	5.877798	-0.026581	2.834013
133.180539	2639.973343	5.882803	-0.026624	2.838010
133.480873	2647.994317	5.887808	-0.026685	2.842018
133.597764	2656.019923	5.892813	-0.026712	2.846012
133.845024	2664.069823	5.897818	-0.026764	2.850020
134.159448	2672.126129	5.902822	-0.026828	2.854029
134.321411	2680.144839	5.907827	-0.026863	2.858005
134.616447	2688.182590	5.912832	-0.026924	2.861992
134.754278	2696.220899	5.917837	-0.026955	2.865966
134.860930	2704.271410	5.922842	-0.026980	2.869938
134.990416	2712.321057	5.927846	-0.027010	2.873905
135.448704	2720.326052	5.932851	-0.027101	2.877863
135.697473	2728.375271	5.937856	-0.027152	2.881826
135.714200	2736.402912	5.942861	-0.027161	2.885760
136.179841	2744.425418	5.947866	-0.027253	2.889711
136.508616	2752.509533	5.952870	-0.027320	2.893678
136.524269	2760.555770	5.957875	-0.027328	2.897605
136.729433	2768.611840	5.962880	-0.027372	2.901542
137.089042	2776.595133	5.967885	-0.027444	2.905446
137.420182	2784.647153	5.972890	-0.027511	2.909376
137.781039	2792.768137	5.977894	-0.027584	2.913337
138.225454	2800.773219	5.982899	-0.027672	2.917240
138.992238	2808.760361	5.987904	-0.027820	2.921146
139.062909	2816.779899	5.992909	-0.027839	2.925026
139.400900	2824.798385	5.997914	-0.027907	2.928914
139.627161	2832.885924	6.002918	-0.027955	2.932824
139.735246	2840.920028	6.007923	-0.027981	2.936697
140.004688	2848.964807	6.012928	-0.028036	2.940579
140.612372	2856.932251	6.017933	-0.028155	2.944436
140.883504	2864.995802	6.022938	-0.028211	2.948316
140.828942	2873.110569	6.027942	-0.028206	2.952199
141.125089	2881.134119	6.032947	-0.028267	2.956051
141.389435	2889.137711	6.037952	-0.028321	2.959887
141.736355	2897.142298	6.042957	-0.028391	2.963723
141.925847	2905.203861	6.047962	-0.028432	2.967573
141.998304	2913.274752	6.052966	-0.028451	2.971416
142.151678	2921.329729	6.057971	-0.028485	2.975251
142.494065	2929.326942	6.062976	-0.028554	2.979063
142.690666	2937.348146	6.067981	-0.028596	2.982874
142.763473	2945.423914	6.072986	-0.028615	2.986699
143.170369	2953.444864	6.077990	-0.028697	2.990511
143.568510	2961.501022	6.082995	-0.028776	2.994334
143.785223	2969.539840	6.088000	-0.028822	2.998135
143.704881	2977.572580	6.093005	-0.028813	3.001913
144.189387	2985.571809	6.098010	-0.028908	3.005699
144.451335	2993.586842	6.103014	-0.028962	3.009476
144.597755	3001.667512	6.108019	-0.028995	3.013274
144.681110	3009.735063	6.113024	-0.029016	3.017057
144.636871	3017.782076	6.118029	-0.029013	3.020820
145.165535	3025.762564	6.123034	-0.029117	3.024575
145.213531	3033.816074	6.128038	-0.029132	3.028336
145.382265	3041.857685	6.133043	-0.029169	3.032093
145.571298	3049.934097	6.138048	-0.029209	3.035862
146.496850	3057.848234	6.143053	-0.029387	3.039587
147.857676	3065.788075	6.148058	-0.029646	3.043339
148.398390	3073.847366	6.153062	-0.029752	3.047103
148.764933	3081.907885	6.158067	-0.029826	3.050855
149.120061	3090.011434	6.163072	-0.029897	3.054621
149.360259	3098.020694	6.168077	-0.029947	3.058333
149.494869	3106.095988	6.173082	-0.029978	3.062066
149.549456	3114.152803	6.178086	-0.029994	3.065783
149.720578	3122.189213	6.183091	-0.030031	3.069491
150.165978	3130.305998	6.188096	-0.030119	3.073244
150.227353	3138.320995	6.193101	-0.030136	3.076928
150.439922	3146.345952	6.198106	-0.030181	3.080619
150.646034	3154.314487	6.203110	-0.030225	3.084280
150.977182	3162.337982	6.208115	-0.030292	3.087967
151.078630	3170.397158	6.213120	-0.030317	3.091655
151.281034	3178.433268	6.218125	-0.030360	3.095333
151.538333	3186.455717	6.223130	-0.030413	3.099003
151.689595	3194.503940	6.228134	-0.030447	3.102676
151.736954	3202.541286	6.233139	-0.030461	3.106334
152.191144	3210.552979	6.238144	-0.030551	3.109995
152.456697	3218.612441	6.243149	-0.030606	3.113664
152.600378	3226.637174	6.248154	-0.030638	3.117308
152.779296	3234.673396	6.253158	-0.030677	3.120955
153.011547	3242.655110	6.258163	-0.030726	3.124575
153.272125	3250.706336	6.263168	-0.030780	3.128223
153.491771	3258.737909	6.268173	-0.030826	3.131857
153.865728	3266.779659	6.273178	-0.030901	3.135497
154.148925	3274.771869	6.278182	-0.030959	3.139107
154.601581	3282.799173	6.283187	-0.031049	3.142736
154.986304	3290.848910	6.288192	-0.031126	3.146368
154.843034	3298.926355	6.293197	-0.031105	3.149985
155.026409	3307.013909	6.298202	-0.031144	3.153616
155.455732	3315.001071	6.303206	-0.031230	3.157209
155.614029	3323.015514	6.308211	-0.031265	3.160799
155.884337	3331.007298	6.313216	-0.031321	3.164379
155.893450	3339.073488	6.318221	-0.031328	3.167977
155.996466	3347.133476	6.323226	-0.031352	3.171572
156.173744	3355.192699	6.328230	-0.031391	3.175165
156.304286	3363.195364	6.333235	-0.031421	3.178728
156.778035	3371.225481	6.338240	-0.031514	3.182313
156.773921	3379.271957	6.343245	-0.031519	3.185881
156.923243	3387.294447	6.348250	-0.031552	3.189441
157.252611	3395.336330	6.353254	-0.031619	3.193014
157.595108	3403.350800	6.358259	-0.031688	3.196570
157.821072	3411.381206	6.363264	-0.031736	3.200125
158.070594	3419.383716	6.368269	-0.031788	3.203664
158.528734	3427.386093	6.373274	-0.031878	3.207208
158.427385	3435.466035	6.378278	-0.031865	3.210759
158.562937	3443.511932	6.383283	-0.031896	3.214301
158.723776	3451.552303	6.388288	-0.031931	3.217838
158.859730	3459.561918	6.393293	-0.031962	3.221356
159.087016	3467.547560	6.398298	-0.032010	3.224864
159.146819	3475.629777	6.403302	-0.032026	3.228403
159.403720	3483.649624	6.408307	-0.032080	3.231919
159.923773	3491.717509	6.413312	-0.032182	3.235462
159.922271	3499.714047	6.418317	-0.032187	3.238950
160.322752	3507.704162	6.423322	-0.032267	3.242447
160.499445	3515.758268	6.428326	-0.032305	3.245960
160.783173	3523.722208	6.433331	-0.032364	3.249433
160.964746	3531.815724	6.438336	-0.032403	3.252955
161.231036	3539.862791	6.443341	-0.032458	3.256456
161.286941	3547.879569	6.448346	-0.032474	3.259932
161.432491	3555.898173	6.453350	-0.032506	3.263409
161.400922	3563.944479	6.458355	-0.032506	3.266887
161.844045	3571.963306	6.463360	-0.032594	3.270368
161.970365	3580.026961	6.468365	-0.032623	3.273852
162.140736	3588.061214	6.473370	-0.032660	3.277322
162.436891	3596.089774	6.478374	-0.032721	3.280790
162.475901	3604.053629	6.483379	-0.032733	3.284217
162.708718	3612.105771	6.488384	-0.032782	3.287685
162.800593	3620.156659	6.493389	-0.032805	3.291144
163.068243	3628.163126	6.498394	-0.032860	3.294587
163.322450	3636.193167	6.503398	-0.032913	3.298036
163.748063	3644.199625	6.508403	-0.032998	3.301478
164.023146	3652.238313	6.513408	-0.033054	3.304924
163.973728	3660.279302	6.518413	-0.033050	3.308355
164.145310	3668.349274	6.523418	-0.033088	3.311803
164.571406	3676.375127	6.528422	-0.033173	3.315238
164.541976	3684.390356	6.533427	-0.033173	3.318649
164.781878	3692.409157	6.538432	-0.033223	3.322067
165.197513	3700.388506	6.543437	-0.033306	3.325471
165.281420	3708.414218	6.548442	-0.033327	3.328880
165.511121	3716.488486	6.553446	-0.033375	3.332310
165.814306	3724.503532	6.558451	-0.033437	3.335715
165.841982	3732.542841	6.563456	-0.033447	3.339117
165.859274	3740.555049	6.568461	-0.033456	3.342503
166.086174	3748.591226	6.573466	-0.033504	3.345903
166.339867	3756.614853	6.578470	-0.033556	3.349296
166.535161	3764.668850	6.583475	-0.033598	3.352696
166.947847	3772.708652	6.588480	-0.033681	3.356094
167.356618	3780.680613	6.593485	-0.033762	3.359460
167.567999	3788.708224	6.598490	-0.033807	3.362839
167.653868	3796.783067	6.603494	-0.033828	3.366230
167.878402	3804.758100	6.608499	-0.033876	3.369581
168.188642	3812.860698	6.613504	-0.033939	3.372984
168.454467	3820.887296	6.618509	-0.033994	3.376351
168.703231	3828.874150	6.623514	-0.034046	3.379697
168.883177	3836.908549	6.628518	-0.034085	3.383057
168.978771	3844.952168	6.633523	-0.034108	3.386415
169.454298	3852.975526	6.638528	-0.034202	3.389774
169.641774	3861.077849	6.643533	-0.034242	3.393153
169.793728	3869.111691	6.648538	-0.034276	3.396499
170.024098	3877.088308	6.653542	-0.034324	3.399820
170.310771	3885.041788	6.658547	-0.034383	3.403130
170.609670	3893.091048	6.663552	-0.034444	3.406477
170.400263	3901.119754	6.668557	-0.034411	3.409795
170.614387	3909.145957	6.673562	-0.034456	3.413123
170.961814	3917.215165	6.678566	-0.034526	3.416470
171.275513	3925.149247	6.683571	-0.034590	3.419757
171.409862	3933.183127	6.688576	-0.034620	3.423076
171.570176	3941.242446	6.693581	-0.034656	3.426402
171.878756	3949.254278	6.698586	-0.034719	3.429711
172.008079	3957.328154	6.703590	-0.034748	3.433037
172.310354	3965.344881	6.708595	-0.034810	3.436341
172.723922	3973.342150	6.713600	-0.034892	3.439638
172.620399	3981.384726	6.718605	-0.034879	3.442933
172.783520	3989.413358	6.723610	-0.034914	3.446228
173.008416	3997.449343	6.728614	-0.034962	3.449524
173.266571	4005.455310	6.733619	-0.035015	3.452807
173.381970	4013.555433	6.738624	-0.035042	3.456120
173.699919	4021.502498	6.743629	-0.035107	3.459374
174.023863	4029.544810	6.748634	-0.035173	3.462664
174.161828	4037.578347	6.753638	-0.035204	3.465941
174.377091	4045.597284	6.758643	-0.035249	3.469212
174.503164	4053.671698	6.763648	-0.035278	3.472499
174.632437	4061.737429	6.768653	-0.035308	3.475780
174.680346	4069.707222	6.773658	-0.035322	3.479016
175.107679	4077.701524	6.778662	-0.035407	3.482271
175.322869	4085.692447	6.783667	-0.035453	3.485514
175.407699	4093.731254	6.788672	-0.035474	3.488770
175.693412	4101.790473	6.793677	-0.035533	3.492038
175.829234	4109.804133	6.798682	-0.035563	3.495279
175.860132	4117.847409	6.803686	-0.035575	3.498526
176.074136	4125.840563	6.808691	-0.035620	3.501755
176.668784	4133.831077	6.813696	-0.035736	3.504992
176.665888	4141.896427	6.818701	-0.035741	3.508238
176.852392	4149.932113	6.823706	-0.035781	3.511475
177.372620	4157.957404	6.828710	-0.035883	3.514714
177.568668	4165.960745	6.833715	-0.035925	3.517932
177.885234	4173.988773	6.838720	-0.035990	3.521161
178.193368	4181.959466	6.843725	-0.036053	3.524363
178.496877	4190.012835	6.848730	-0.036115	3.527595
178.537034	4198.105461	6.853734	-0.036128	3.530832
178.679063	4206.123539	6.858739	-0.036159	3.534039
178.977459	4214.148113	6.863744	-0.036220	3.537251
178.843773	4222.193111	6.868749	-0.036201	3.540455
178.946898	4230.188335	6.873754	-0.036226	3.543643
179.294983	4238.234439	6.878758	-0.036296	3.546856
179.226111	4246.261069	6.883763	-0.036289	3.550045
179.395891	4254.396590	6.888768	-0.036326	3.553283
179.781152	4262.397677	6.893773	-0.036403	3.556470
179.878585	4270.357389	6.898778	-0.036426	3.559629
180.016342	4278.360654	6.903782	-0.036458	3.562804
180.109618	4286.370468	6.908787	-0.036480	3.565978
180.469448	4294.354415	6.913792	-0.036553	3.569146
180.782368	4302.421001	6.918797	-0.036616	3.572343
181.069689	4310.454908	6.923802	-0.036675	3.575523
181.049854	4318.475781	6.928806	-0.036677	3.578686
181.381248	4326.455178	6.933811	-0.036744	3.581840
181.654336	4334.480112	6.938816	-0.036801	3.585008
181.842039	4342.539900	6.943821	-0.036841	3.588184
182.033005	4350.543112	6.948826	-0.036882	3.591335
182.226703	4358.581883	6.953830	-0.036924	3.594497
182.161113	4366.576411	6.958835	-0.036917	3.597632
182.403055	4374.629944	6.963840	-0.036967	3.600796
182.578910	4382.598110	6.968845	-0.037005	3.603922
182.933583	4390.610817	6.973850	-0.037077	3.607067
183.217312	4398.660495	6.978854	-0.037135	3.610222
183.188877	4406.713098	6.983859	-0.037135	3.613367
183.717720	4414.762117	6.988864	-0.037239	3.616523
183.737472	4422.756591	6.993869	-0.037248	3.619641
184.118581	4430.757417	6.998874	-0.037325	3.622768
184.109968	4438.805502	7.003878	-0.037329	3.625901
184.034556	4446.825872	7.008883	-0.037320	3.629018
184.535108	4454.903773	7.013888	-0.037419	3.632171
184.760698	4462.932427	7.018893	-0.037466	3.635294
184.745797	4470.939681	7.023898	-0.037469	3.638400
185.173598	4478.972323	7.028902	-0.037554	3.641525
185.163252	4486.920487	7.033907	-0.037558	3.644603
185.034582	4495.007015	7.038912	-0.037539	3.647728
185.362458	4503.003682	7.043917	-0.037606	3.650828
185.615341	4511.041539	7.048922	-0.037658	3.653940
185.929027	4519.072510	7.053926	-0.037722	3.657047
186.051908	4527.052152	7.058931	-0.037750	3.660127
186.361562	4535.112661	7.063936	-0.037813	3.663241
186.471737	4543.148220	7.068941	-0.037839	3.666337
186.612793	4551.156063	7.073946	-0.037871	3.669421
186.826716	4559.198327	7.078950	-0.037916	3.672517
187.104615	4567.196014	7.083955	-0.037974	3.675595
187.191378	4575.221447	7.088960	-0.037995	3.678676
187.249136	4583.251513	7.093965	-0.038011	3.681755
187.465824	4591.233741	7.098970	-0.038057	3.684818
187.849507	4599.258994	7.103974	-0.038134	3.687899
187.874313	4607.302580	7.108979	-0.038144	3.690975
188.097403	4615.345563	7.113984	-0.038191	3.694053
188.295925	4623.360972	7.118989	-0.038234	3.697118
188.412173	4631.368039	7.123994	-0.038261	3.700174
188.611246	4639.416542	7.128998	-0.038303	3.703247
188.883321	4647.401452	7.134003	-0.038359	3.706294
189.138411	4655.433569	7.139008	-0.038412	3.709356
189.087258	4663.525115	7.144013	-0.038408	3.712430
189.213165	4671.583156	7.149018	-0.038437	3.715494
189.710802	4679.528547	7.154022	-0.038535	3.718521
189.981332	4687.520728	7.159027	-0.038591	3.721558
190.272721	4695.507515	7.164032	-0.038651	3.724591
190.504102	4703.550973	7.169037	-0.038699	3.727642
190.436792	4711.602757	7.174042	-0.038692	3.730686
190.571035	4719.648335	7.179046	-0.038723	3.733730
190.762655	4727.633240	7.184051	-0.038764	3.736750
190.970437	4735.648511	7.189056	-0.038808	3.739779
191.082268	4743.663972	7.194061	-0.038834	3.742804
191.346918	4751.678077	7.199066	-0.038889	3.745829
191.743486	4759.727072	7.204070	-0.038968	3.748868
191.667151	4767.786421	7.209075	-0.038959	3.751897
191.758469	4775.827744	7.214080	-0.038982	3.754921
192.044156	4783.819510	7.219085	-0.039040	3.757928
192.182078	4791.831900	7.224090	-0.039072	3.760938
192.369560	4799.850235	7.229094	-0.039112	3.763948
192.622984	4807.871879	7.234099	-0.039165	3.766959
192.845745	4815.900259	7.239104	-0.039212	3.769968
192.801853	4823.990619	7.244109	-0.039209	3.772993
193.095007	4831.978444	7.249114	-0.039269	3.775985
193.389202	4839.968494	7.254118	-0.039329	3.778974
193.395557	4847.999075	7.259123	-0.039336	3.781971
193.706688	4855.996805	7.264128	-0.039399	3.784959
193.954845	4864.045013	7.269133	-0.039451	3.787962
193.959570	4872.043744	7.274138	-0.039457	3.790940
194.163940	4880.136011	7.279142	-0.039501	3.793954
194.182695	4888.130654	7.284147	-0.039510	3.796925
194.419170	4896.099378	7.289152	-0.039559	3.799889
194.742431	4904.097108	7.294157	-0.039625	3.802863
194.799763	4912.121895	7.299162	-0.039641	3.805839
195.104341	4920.165529	7.304166	-0.039703	3.808825
195.160987	4928.195459	7.309171	-0.039719	3.811799
195.260819	4936.244385	7.314176	-0.039743	3.814778
195.516200	4944.245863	7.319181	-0.039796	3.817740
195.647230	4952.217709	7.324186	-0.039826	3.820687
195.937199	4960.250970	7.329190	-0.039885	3.823657
196.106561	4968.281423	7.334195	-0.039922	3.826622
196.261068	4976.296990	7.339200	-0.039956	3.829578
196.448973	4984.362741	7.344205	-0.039997	3.832551
196.600347	4992.360496	7.349210	-0.040031	3.835496
196.914445	5000.363777	7.354214	-0.040094	3.838444
196.878435	5008.417725	7.359219	-0.040093	3.841401
197.004425	5016.392188	7.364224	-0.040122	3.844330
197.370720	5024.437717	7.369229	-0.040196	3.847288
197.554989	5032.430703	7.374234	-0.040236	3.850220
197.652432	5040.544732	7.379238	-0.040259	3.853193
197.627413	5048.549773	7.384243	-0.040260	3.856121
197.904874	5056.533968	7.389248	-0.040317	3.859046
197.904338	5064.557573	7.394253	-0.040322	3.861977
197.914568	5072.581558	7.399258	-0.040330	3.864906
198.246269	5080.607807	7.404262	-0.040397	3.867840
198.551565	5088.640880	7.409267	-0.040459	3.870774
198.583374	5096.936847	7.414272	-0.040471	3.873795
198.699539	5104.866557	7.419277	-0.040498	3.876683
199.127711	5112.729633	7.424282	-0.040583	3.879551
199.243210	5120.771046	7.429286	-0.040610	3.882475
199.201729	5128.726313	7.434291	-0.040608	3.885362
199.615177	5136.735606	7.439296	-0.040690	3.888276
199.856288	5144.794683	7.444301	-0.040740	3.891202
200.122557	5152.799122	7.449306	-0.040795	3.894107
200.377932	5160.828350	7.454310	-0.040848	3.897018
200.455256	5168.807407	7.459315	-0.040868	3.899906
200.362133	5176.876494	7.464320	-0.040856	3.902821
200.521214	5184.872742	7.469325	-0.040891	3.905712
200.910246	5192.855286	7.474330	-0.040969	3.908600
200.961500	5200.966136	7.479334	-0.040984	3.911526
201.121026	5208.947518	7.484339	-0.041019	3.914405
201.367344	5216.959893	7.489344	-0.041071	3.917294
201.731151	5224.960150	7.494349	-0.041144	3.920180
201.552600	5232.945397	7.499354	-0.041116	3.923048
201.871682	5241.006832	7.504358	-0.041181	3.925950
202.075716	5248.974052	7.509363	-0.041224	3.928814
202.221412	5257.074602	7.514368	-0.041257	3.931723
202.372751	5265.089462	7.519373	-0.041291	3.934599
202.556932	5273.070259	7.524378	-0.041330	3.937461
202.768092	5281.112321	7.529382	-0.041375	3.940344
202.942288	5289.094095	7.534387	-0.041413	3.943202
203.177415	5297.145144	7.539392	-0.041462	3.946084
203.152225	5305.191357	7.544397	-0.041463	3.948957
203.240508	5313.220379	7.549402	-0.041485	3.951824
203.471603	5321.263208	7.554406	-0.041533	3.954697
203.784792	5329.234399	7.559411	-0.041597	3.957543
203.801727	5337.236304	7.564416	-0.041606	3.960393
203.957201	5345.245221	7.569421	-0.041640	3.963246
204.298510	5353.266005	7.574426	-0.041709	3.966105
204.276235	5361.303051	7.579430	-0.041710	3.968960
204.223399	5369.313916	7.584435	-0.041706	3.971804
204.693559	5377.369998	7.589440	-0.041799	3.974671
205.021213	5385.385095	7.594445	-0.041866	3.977518
204.872920	5393.348220	7.599450	-0.041843	3.980337
205.466445	5401.382802	7.604454	-0.041959	3.983192
205.396935	5409.411912	7.609459	-0.041952	3.986032
205.667991	5417.452134	7.614464	-0.042008	3.988879
205.757955	5425.510120	7.619469	-0.042030	3.991728
205.991775	5433.530142	7.624474	-0.042079	3.994563
206.169443	5441.575358	7.629478	-0.042117	3.997404
206.268852	5449.494416	7.634483	-0.042141	4.000198
206.354105	5457.535827	7.639488	-0.042163	4.003032
206.434306	5465.576113	7.644493	-0.042183	4.005864
206.664966	5473.570974	7.649498	-0.042231	4.008681
206.887857	5481.629652	7.654502	-0.042278	4.011517
207.173271	5489.662010	7.659507	-0.042337	4.014344
207.390763	5497.676486	7.664512	-0.042383	4.017161
207.508520	5505.690415	7.669517	-0.042410	4.019974
207.954867	5513.671493	7.674522	-0.042499	4.022779
208.195920	5521.720825	7.679526	-0.042549	4.025602
208.008538	5529.736626	7.684531	-0.042520	4.028406
208.613445	5537.775300	7.689536	-0.042638	4.031227
208.725142	5545.918923	7.694541	-0.042664	4.034076
208.736695	5553.871513	7.699546	-0.042672	4.036854
208.927169	5561.843397	7.704550	-0.042713	4.039640
208.971390	5569.819053	7.709555	-0.042726	4.042422
209.242575	5577.830011	7.714560	-0.042782	4.045219
209.211060	5585.871983	7.719565	-0.042782	4.048020
209.360607	5593.897545	7.724570	-0.042815	4.050816
209.682486	5601.923300	7.729574	-0.042881	4.053613
209.809604	5609.942198	7.734579	-0.042910	4.056403
210.127029	5617.908435	7.739584	-0.042974	4.059175
210.284419	5625.923752	7.744589	-0.043009	4.061959
210.350144	5633.923204	7.749594	-0.043027	4.064735
210.532311	5641.992762	7.754598	-0.043066	4.067536
210.764067	5649.981207	7.759603	-0.043115	4.070306
211.071257	5658.004617	7.764608	-0.043177	4.073088
211.137081	5666.095742	7.769613	-0.043195	4.075888
211.357687	5674.036298	7.774618	-0.043241	4.078637
211.637721	5682.116435	7.779622	-0.043299	4.081432
211.323880	5690.064822	7.784627	-0.043246	4.084172
211.568027	5698.135756	7.789632	-0.043297	4.086960
211.794344	5706.098878	7.794637	-0.043345	4.089709
211.782309	5714.159279	7.799642	-0.043348	4.092486
212.007343	5722.189616	7.804646	-0.043395	4.095254
212.089258	5730.182022	7.809651	-0.043416	4.098005
212.251421	5738.225792	7.814656	-0.043452	4.100773
212.461351	5746.215068	7.819661	-0.043496	4.103521
212.498519	5754.237312	7.824666	-0.043508	4.106276
212.908836	5762.272632	7.829670	-0.043590	4.109039
213.045506	5770.294738	7.834675	-0.043621	4.111791
213.226555	5778.347045	7.839680	-0.043660	4.114553
213.481835	5786.388389	7.844685	-0.043713	4.117310
213.495050	5794.315570	7.849690	-0.043721	4.120023
213.633984	5802.349265	7.854694	-0.043753	4.122772
213.900674	5810.364493	7.859699	-0.043808	4.125515
214.006587	5818.416666	7.864704	-0.043833	4.128266
214.128838	5826.456282	7.869709	-0.043861	4.131012
214.242058	5834.464091	7.874714	-0.043888	4.133745
214.491557	5842.518154	7.879718	-0.043939	4.136493
214.576944	5850.521221	7.884723	-0.043961	4.139220
214.847784	5858.563366	7.889728	-0.044017	4.141961
215.002210	5866.504915	7.894733	-0.044051	4.144664
215.137077	5874.502937	7.899738	-0.044081	4.147385
215.126188	5882.632734	7.904742	-0.044085	4.150146
215.459794	5890.608749	7.909747	-0.044152	4.152858
215.773949	5898.625776	7.914752	-0.044216	4.155582
215.705279	5906.669694	7.919757	-0.044209	4.158308
215.762463	5914.676763	7.924762	-0.044225	4.161022
216.101558	5922.641662	7.929766	-0.044294	4.163723
216.043370	5930.684418	7.934771	-0.044288	4.166443
216.250315	5938.680993	7.939776	-0.044332	4.169150
216.528163	5946.719296	7.944781	-0.044389	4.171869
216.568007	5954.755176	7.949786	-0.044402	4.174584
216.784581	5962.784904	7.954790	-0.044448	4.177296
216.677026	5970.733396	7.959795	-0.044434	4.179976
216.976844	5978.782022	7.964800	-0.044495	4.182692
217.182705	5986.796419	7.969805	-0.044539	4.185394
217.182637	5994.813471	7.974810	-0.044544	4.188092
217.454000	6002.878035	7.979814	-0.044600	4.190808
217.696167	6010.953529	7.984819	-0.044651	4.193526
217.757859	6018.967592	7.989824	-0.044668	4.196219
218.056669	6026.900285	7.994829	-0.044729	4.198885
218.218573	6034.883399	7.999834	-0.044764	4.201565
218.316872	6042.909993	8.004838	-0.044788	4.204258
218.607316	6050.919982	8.009843	-0.044847	4.206945
218.752073	6058.907065	8.014848	-0.044880	4.209621
218.992145	6066.989699	8.019853	-0.044930	4.212328
219.006537	6074.984586	8.024858	-0.044938	4.215002
219.269001	6083.047149	8.029862	-0.044992	4.217700
219.295324	6090.986502	8.034867	-0.045003	4.220352
219.562808	6099.029397	8.039872	-0.045058	4.223039
219.838101	6107.041726	8.044877	-0.045115	4.225715
219.939994	6115.044685	8.049882	-0.045139	4.228384
220.022821	6123.090801	8.054886	-0.045160	4.231065
220.257278	6131.108584	8.059891	-0.045209	4.233737
220.318030	6139.181596	8.064896	-0.045226	4.236424
220.535025	6147.120989	8.069901	-0.045272	4.239066
220.549801	6155.155764	8.074906	-0.045280	4.241736
220.719880	6163.153612	8.079910	-0.045317	4.244394
220.820197	6171.210260	8.084915	-0.045341	4.247069
220.933030	6179.216137	8.089920	-0.045368	4.249726
221.337994	6187.268926	8.094925	-0.045449	4.252399
221.447812	6195.260589	8.099930	-0.045474	4.255047
221.585142	6203.303699	8.104934	-0.045505	4.257711
221.515185	6211.258415	8.109939	-0.045498	4.260342
221.860924	6219.293741	8.114944	-0.045568	4.263002
222.034103	6227.311433	8.119949	-0.045605	4.265653
221.870804	6235.362971	8.124954	-0.045580	4.268311
222.086130	6243.412344	8.129958	-0.045626	4.270969
222.298781	6251.492464	8.134963	-0.045671	4.273636
222.459431	6259.452112	8.139968	-0.045706	4.276261
222.559270	6267.465691	8.144973	-0.045730	4.278901
222.815115	6275.428109	8.149978	-0.045783	4.281525
223.181766	6283.431633	8.154982	-0.045857	4.284161
223.039506	6291.482483	8.159987	-0.045836	4.286807
223.274717	6299.487023	8.164992	-0.045885	4.289439
223.642949	6307.518015	8.169997	-0.045959	4.292079
223.585280	6315.487491	8.175002	-0.045954	4.294694
223.968584	6323.591034	8.180006	-0.046031	4.297355
224.085451	6331.567098	8.185011	-0.046058	4.299971
224.106763	6339.583731	8.190016	-0.046068	4.302597
224.058757	6347.599296	8.195021	-0.046064	4.305221
224.282512	6355.613329	8.200026	-0.046111	4.307844
224.515538	6363.665559	8.205030	-0.046160	4.310479
224.557831	6371.675634	8.210035	-0.046173	4.313097
224.972887	6379.726971	8.215040	-0.046256	4.315729
225.098880	6387.685694	8.220045	-0.046285	4.318328
224.925250	6395.702001	8.225050	-0.046258	4.320941
225.018146	6403.730538	8.230054	-0.046281	4.323559
225.342062	6411.735844	8.235059	-0.046347	4.326169
225.550212	6419.724694	8.240064	-0.046391	4.328772
225.492870	6427.832696	8.245069	-0.046386	4.331409
225.839187	6435.785152	8.250074	-0.046455	4.333998
226.108425	6443.888305	8.255078	-0.046511	4.336633
225.891364	6451.805877	8.260083	-0.046476	4.339203
226.296618	6459.850616	8.265088	-0.046557	4.341817
226.508569	6467.831242	8.270093	-0.046602	4.344408
226.539410	6475.894639	8.275098	-0.046613	4.347022
226.667283	6483.870323	8.280102	-0.046642	4.349607
226.892253	6491.933711	8.285107	-0.046690	4.352219
227.315148	6500.043426	8.290112	-0.046774	4.354847
227.460786	6508.017922	8.295117	-0.046806	4.357427
227.607599	6515.948878	8.300122	-0.046839	4.359991
227.768848	6523.947127	8.305126	-0.046875	4.362576
227.786669	6531.965536	8.310131	-0.046883	4.365165
228.060482	6539.966407	8.315136	-0.046940	4.367748
228.385418	6548.002156	8.320141	-0.047006	4.370341
228.306877	6556.029049	8.325146	-0.046997	4.372927
228.479619	6564.074440	8.330150	-0.047034	4.375519
228.736779	6572.050364	8.335155	-0.047088	4.378088
229.067618	6580.046251	8.340160	-0.047155	4.380662
229.126913	6588.101393	8.345165	-0.047171	4.383252
229.277850	6596.074172	8.350170	-0.047205	4.385815
229.509970	6604.153347	8.355174	-0.047253	4.388410
229.693567	6612.113689	8.360179	-0.047293	4.390966
229.652760	6620.220865	8.365184	-0.047291	4.393566
229.925059	6628.242762	8.370189	-0.047347	4.396139
229.984333	6636.184337	8.375194	-0.047363	4.398683
230.143152	6644.203023	8.380198	-0.047398	4.401251
230.273510	6652.186914	8.385203	-0.047428	4.403807
230.209752	6660.287043	8.390208	-0.047422	4.406397
230.197019	6668.284597	8.395213	-0.047425	4.408953
230.356218	6676.277235	8.400218	-0.047460	4.411507
230.775156	6684.341936	8.405222	-0.047543	4.414083
230.762354	6692.404473	8.410227	-0.047547	4.416655
230.938336	6700.369921	8.415232	-0.047585	4.419196
231.207913	6708.420943	8.420237	-0.047640	4.421763
231.171544	6716.352842	8.425242	-0.047639	4.424289
231.273928	6724.395160	8.430246	-0.047664	4.426849
231.424217	6732.388481	8.435251	-0.047697	4.429393
231.434425	6740.433642	8.440256	-0.047704	4.431951
231.742835	6748.512691	8.445261	-0.047767	4.434519
231.788816	6756.501849	8.450266	-0.047781	4.437056
232.231113	6764.487243	8.455270	-0.047869	4.439593
232.254827	6772.498774	8.460275	-0.047879	4.442134
232.266137	6780.460894	8.465280	-0.047886	4.444658
232.645402	6788.550879	8.470285	-0.047962	4.447223
232.706693	6796.537356	8.475290	-0.047979	4.449752
232.896936	6804.627429	8.480294	-0.048020	4.452313
232.985522	6812.629712	8.485299	-0.048042	4.454844
233.294202	6820.624004	8.490304	-0.048105	4.457373
233.368652	6828.630742	8.495309	-0.048124	4.459902
233.373335	6836.652784	8.500314	-0.048131	4.462435
233.500351	6844.618583	8.505318	-0.048160	4.464949
233.446373	6852.671222	8.510323	-0.048155	4.467489
233.590410	6860.646925	8.515328	-0.048187	4.470003
234.094505	6868.753043	8.520333	-0.048287	4.472559
234.197229	6876.705719	8.525338	-0.048311	4.475063
234.140993	6884.774769	8.530342	-0.048306	4.477602
234.315779	6892.752605	8.535347	-0.048344	4.480111
234.411858	6900.762632	8.540352	-0.048368	4.482629
234.732158	6908.782885	8.545357	-0.048433	4.485149
234.744922	6916.779015	8.550362	-0.048441	4.487660
234.738607	6924.791766	8.555366	-0.048445	4.490174
235.135462	6932.855943	8.560371	-0.048524	4.492704
235.186665	6940.865298	8.565376	-0.048539	4.495214
235.485566	6948.891839	8.570381	-0.048600	4.497729
235.380296	6956.830868	8.575386	-0.048586	4.500215
235.467376	6964.889336	8.580391	-0.048608	4.502736
235.490270	6972.873025	8.585395	-0.048617	4.505233
235.761017	6980.934016	8.590400	-0.048673	4.507753
236.008336	6988.959836	8.595405	-0.048725	4.510261
235.980476	6997.005436	8.600410	-0.048725	4.512772
236.353244	7005.065397	8.605415	-0.048800	4.515288
236.449953	7012.999920	8.610419	-0.048823	4.517762
236.488820	7020.978347	8.615424	-0.048836	4.520249
236.855973	7029.033005	8.620429	-0.048910	4.522759
237.100793	7036.971773	8.625434	-0.048961	4.525231
236.944842	7045.012074	8.630439	-0.048937	4.527732
237.167706	7053.026131	8.635443	-0.048984	4.530225
237.242411	7061.079817	8.640448	-0.049004	4.532728
237.386234	7069.131528	8.645453	-0.049036	4.535229
237.539246	7077.095150	8.650458	-0.049070	4.537702
237.702952	7085.117469	8.655463	-0.049106	4.540192
237.964633	7093.141694	8.660467	-0.049160	4.542680
238.088727	7101.118790	8.665472	-0.049188	4.545153
238.109729	7109.186523	8.670477	-0.049198	4.547652
238.216202	7117.153372	8.675482	-0.049223	4.550119
238.265602	7125.251028	8.680487	-0.049238	4.552625
238.381661	7133.233704	8.685491	-0.049265	4.555093
238.584218	7141.248664	8.690496	-0.049308	4.557571
238.827356	7149.226451	8.695501	-0.049359	4.560036
238.809199	7157.231986	8.700506	-0.049361	4.562508
238.989071	7165.246145	8.705511	-0.049400	4.564981
238.986627	7173.290724	8.710515	-0.049405	4.567462
239.149210	7181.251973	8.715520	-0.049440	4.569916
239.432267	7189.359083	8.720525	-0.049498	4.572414
239.587165	7197.367698	8.725530	-0.049533	4.574880
239.859881	7205.390504	8.730535	-0.049589	4.577349
239.773148	7213.362905	8.735539	-0.049578	4.579801
240.114314	7221.431916	8.740544	-0.049647	4.582282
240.319197	7229.433598	8.745549	-0.049691	4.584741
240.220210	7237.456595	8.750554	-0.049678	4.587204
240.306100	7245.413300	8.755559	-0.049699	4.589646
240.637314	7253.504159	8.760563	-0.049766	4.592128
240.897920	7261.528343	8.765568	-0.049820	4.594588
241.106221	7269.564144	8.770573	-0.049865	4.597051
241.252433	7277.487149	8.775578	-0.049897	4.599477
241.289904	7285.557349	8.780583	-0.049910	4.601947
241.176235	7293.508511	8.785587	-0.049894	4.604380
241.333019	7301.569896	8.790592	-0.049929	4.606844
241.654272	7309.549759	8.795597	-0.049994	4.609283
241.670861	7317.598465	8.800602	-0.050002	4.611741
241.971115	7325.619757	8.805607	-0.050064	4.614190
242.172950	7333.691481	8.810611	-0.050107	4.616652
242.178082	7341.659998	8.815616	-0.050113	4.619082
242.429340	7349.683066	8.820621	-0.050165	4.621527
242.573039	7357.642745	8.825626	-0.050198	4.623952
242.821008	7365.684720	8.830631	-0.050249	4.626400
242.783130	7373.666079	8.835635	-0.050248	4.628829
242.986791	7381.747440	8.840640	-0.050291	4.631287
243.285657	7389.791204	8.845645	-0.050352	4.633731
243.134961	7397.745025	8.850650	-0.050330	4.636148
243.357555	7405.731429	8.855655	-0.050376	4.638573
243.637138	7413.782939	8.860659	-0.050434	4.641016
243.674331	7421.745589	8.865664	-0.050446	4.643431
243.803790	7429.851702	8.870669	-0.050476	4.645888
243.832415	7437.859859	8.875674	-0.050487	4.648315
244.089238	7445.864630	8.880679	-0.050540	4.650739
244.064179	7453.910989	8.885683	-0.050541	4.653174
243.976711	7461.883937	8.890688	-0.050530	4.655586
244.276903	7469.870604	8.895693	-0.050591	4.658001
244.649174	7477.862836	8.900698	-0.050666	4.660416
244.604362	7485.923925	8.905703	-0.050663	4.662851
244.742488	7493.926859	8.910707	-0.050694	4.665266
244.843915	7501.913148	8.915712	-0.050719	4.667676
245.167359	7509.970871	8.920717	-0.050784	4.670106
245.101461	7518.068415	8.925722	-0.050777	4.672546
245.258595	7526.119425	8.930727	-0.050812	4.674971
245.443872	7534.063851	8.935731	-0.050852	4.677363
245.710316	7541.984830	8.940736	-0.050907	4.679747
245.668185	7550.043253	8.945741	-0.050905	4.682171
245.900353	7557.981695	8.950746	-0.050953	4.684557
245.951372	7566.058337	8.955751	-0.050968	4.686983
246.062841	7574.050130	8.960755	-0.050994	4.689383
246.238560	7582.113051	8.965760	-0.051033	4.691803
246.144132	7590.135806	8.970765	-0.051021	4.694210
246.292430	7598.128840	8.975770	-0.051054	4.696607
246.746893	7606.111428	8.980775	-0.051144	4.698998
246.654103	7614.115297	8.985779	-0.051132	4.701396
246.896389	7622.126671	8.990784	-0.051182	4.703794
246.988965	7630.194355	8.995789	-0.051205	4.706208
247.001624	7638.190444	9.000794	-0.051213	4.708599
247.302698	7646.202249	9.005799	-0.051274	4.710993
247.168987	7654.280646	9.010803	-0.051255	4.713407
247.398362	7662.283486	9.015808	-0.051303	4.715797
247.694320	7670.304637	9.020813	-0.051364	4.718190
247.711119	7678.233389	9.025818	-0.051372	4.720555
247.719180	7686.278119	9.030823	-0.051379	4.722954
247.766181	7694.305294	9.035827	-0.051393	4.725346
247.991428	7702.349719	9.040832	-0.051441	4.727741
248.303005	7710.369754	9.045837	-0.051504	4.730128
248.316168	7718.408972	9.050842	-0.051512	4.732520
248.432147	7726.414417	9.055847	-0.051539	4.734901
248.578161	7734.438950	9.060851	-0.051572	4.737286
248.646122	7742.398482	9.065856	-0.051590	4.739650
248.761933	7750.466625	9.070861	-0.051617	4.742046
248.959562	7758.437701	9.075866	-0.051659	4.744411
249.114028	7766.457642	9.080871	-0.051693	4.746790
249.107098	7774.451482	9.085875	-0.051697	4.749160
249.266415	7782.544944	9.090880	-0.051733	4.751558
249.457806	7790.561746	9.095885	-0.051774	4.753932
249.525197	7798.571724	9.100890	-0.051792	4.756303
249.596045	7806.544616	9.105895	-0.051810	4.758662
249.853791	7814.555388	9.110899	-0.051864	4.761030
250.179648	7822.537272	9.115904	-0.051930	4.763389
250.171337	7830.559319	9.120909	-0.051934	4.765759
250.095054	7838.554912	9.125914	-0.051925	4.768121
250.258362	7846.593443	9.130919	-0.051961	4.770493
250.301120	7854.650378	9.135923	-0.051974	4.772869
250.443164	7862.649105	9.140928	-0.052006	4.775227
250.694425	7870.686136	9.145933	-0.052058	4.777595
250.900202	7878.627001	9.150938	-0.052102	4.779934
250.991418	7886.633921	9.155943	-0.052125	4.782291
251.210628	7894.696472	9.160947	-0.052171	4.784662
251.510335	7902.642150	9.165952	-0.052232	4.786998
251.546048	7910.698557	9.170957	-0.052244	4.789367
251.437856	7918.709083	9.175962	-0.052229	4.791721
251.522592	7926.785868	9.180967	-0.052251	4.794093
251.691013	7934.815804	9.185971	-0.052288	4.796449
252.005369	7942.752964	9.190976	-0.052351	4.798777
252.299751	7950.827972	9.195981	-0.052412	4.801143
252.212461	7958.757403	9.200986	-0.052401	4.803468
252.482084	7966.817708	9.205991	-0.052457	4.805828
252.473123	7974.838245	9.210995	-0.052460	4.808177
252.628155	7982.846117	9.216000	-0.052495	4.810520
252.765498	7990.271649	9.221005	-0.052525	4.812692
252.793072	7994.739895	9.226010	-0.052534	4.813998

253.107282	7997.306681	9.231015	-0.052594	4.814747
253.334393	7998.620761	9.236019	-0.052637	4.815130
253.231625	7999.048436	9.241024	-0.052619	4.815256
253.306961	8000.035488	9.246029	-0.052634	4.815544
253.260641	7999.986687	9.251034	-0.052625	4.815530
253.661603	7999.998603	9.256039	-0.052700	4.815532
253.633420	8000.060110	9.261043	-0.052695	4.815550
253.707063	8000.003658	9.266048	-0.052709	4.815533
253.767444	8000.038844	9.271053	-0.052720	4.815543
253.695265	7999.998164	9.276058	-0.052707	4.815531
253.788953	8000.030690	9.281063	-0.052725	4.815540
253.786592	8000.027466	9.286067	-0.052725	4.815539
253.757469	8000.013125	9.291072	-0.052719	4.815535
253.839672	8000.056144	9.296077	-0.052735	4.815547
254.033555	7999.987773	9.301082	-0.052771	4.815527
254.182458	8000.038292	9.306087	-0.052799	4.815541
254.135607	8000.014047	9.311091	-0.052791	4.815534
254.155327	7999.959917	9.316096	-0.052795	4.815518
254.331673	8000.073903	9.321101	-0.052828	4.815550
253.957924	8000.056059	9.326106	-0.052758	4.815547
254.021328	8000.058184	9.331111	-0.052770	4.815547
254.242531	8000.051141	9.336115	-0.052812	4.815544
254.144342	8000.053827	9.341120	-0.052794	4.815545
254.246170	8000.036286	9.346125	-0.052813	4.815540
254.245160	8000.021336	9.351130	-0.052813	4.815535
254.283269	8000.034796	9.356135	-0.052820	4.815539
254.435504	8000.091779	9.361139	-0.052849	4.815555
254.329819	8000.087933	9.366144	-0.052829	4.815554
254.618190	8000.096944	9.371149	-0.052883	4.815556
254.221810	8000.047754	9.376154	-0.052810	4.815543
254.547546	8000.077669	9.381159	-0.052871	4.815550
254.463904	8000.063503	9.386163	-0.052855	4.815547
254.463025	8000.085938	9.391168	-0.052855	4.815553
254.444085	8000.088852	9.396173	-0.052852	4.815554
254.518428	8000.042023	9.401178	-0.052866	4.815540
254.612610	8000.068150	9.406183	-0.052884	4.815547
254.566396	8000.079163	9.411187	-0.052875	4.815551
254.506136	8000.046153	9.416192	-0.052864	4.815541
254.793782	8000.090399	9.421197	-0.052918	4.815553
254.561394	8000.028938	9.426202	-0.052875	4.815536
254.679688	8000.074686	9.431207	-0.052897	4.815549
254.888111	8000.081320	9.436211	-0.052936	4.815550
254.752602	8000.027853	9.441216	-0.052911	4.815535
254.777677	8000.082757	9.446221	-0.052916	4.815551
254.659481	8000.023164	9.451226	-0.052895	4.815534
254.859663	8000.033936	9.456231	-0.052932	4.815536
254.708403	8000.101976	9.461235	-0.052904	4.815557
254.581244	8000.035828	9.466240	-0.052881	4.815538
254.786729	8000.088343	9.471245	-0.052919	4.815552
254.865414	8000.058675	9.476250	-0.052934	4.815543
254.681041	8000.111219	9.481255	-0.052900	4.815559
254.810065	8000.078102	9.486259	-0.052924	4.815549
254.958702	8000.047443	9.491264	-0.052952	4.815539
255.022590	8000.053848	9.496269	-0.052964	4.815541
254.964317	8000.036892	9.501274	-0.052954	4.815536
254.920416	8000.068237	9.506279	-0.052946	4.815546
254.940288	8000.089944	9.511283	-0.052950	4.815552
255.070712	8000.076076	9.516288	-0.052974	4.815547
255.261766	8000.142242	9.521293	-0.053010	4.815566
255.012107	8000.060203	9.526298	-0.052964	4.815543
255.091682	8000.097840	9.531303	-0.052979	4.815553
254.942230	8000.083665	9.536307	-0.052951	4.815550
255.038530	8000.073511	9.541312	-0.052969	4.815547
255.072048	8000.118940	9.546317	-0.052976	4.815560
254.947433	8000.104103	9.551322	-0.052953	4.815556
255.077531	8000.093434	9.556327	-0.052977	4.815552
255.094025	8000.115086	9.561331	-0.052980	4.815558
254.919247	8000.098359	9.566336	-0.052948	4.815554
255.187769	8000.119864	9.571341	-0.052998	4.815559
254.874725	8000.070967	9.576346	-0.052940	4.815547
255.152966	8000.115061	9.581351	-0.052992	4.815558
255.143704	8000.070067	9.586355	-0.052991	4.815545
255.129869	8000.036749	9.591360	-0.052988	4.815535
255.242898	8000.112319	9.596365	-0.053010	4.815557
255.049330	8000.030129	9.601370	-0.052974	4.815534
255.058619	8000.081570	9.606375	-0.052976	4.815549
255.188069	8000.083709	9.611379	-0.053000	4.815549
254.959895	8000.098152	9.616384	-0.052958	4.815554
255.090349	8000.135555	9.621389	-0.052982	4.815564
255.033959	8000.082313	9.626394	-0.052972	4.815549
255.127987	8000.092417	9.631399	-0.052990	4.815552
255.216582	8000.090682	9.636403	-0.053007	4.815551
255.249504	8000.074150	9.641408	-0.053013	4.815546
255.169908	8000.094229	9.646413	-0.052998	4.815552
255.080102	8000.074621	9.651418	-0.052982	4.815547
255.193392	8000.067950	9.656423	-0.053003	4.815544
255.386752	8000.059385	9.661427	-0.053039	4.815541
255.090234	7999.989396	9.666432	-0.052984	4.815522
255.348666	8000.041710	9.671437	-0.053033	4.815536
255.405334	8000.082178	9.676442	-0.053043	4.815547
255.302505	8000.108286	9.681447	-0.053025	4.815555
255.266402	8000.074602	9.686451	-0.053018	4.815546
255.227557	8000.061169	9.691456	-0.053011	4.815542
255.295187	8000.098611	9.696461	-0.053024	4.815552
255.159454	8000.094273	9.701466	-0.052999	4.815552
255.318039	8000.095820	9.706471	-0.053029	4.815552
255.410016	8000.078119	9.711475	-0.053046	4.815546
255.263127	8000.065053	9.716480	-0.053019	4.815543
255.371100	8000.073248	9.721485	-0.053039	4.815545
255.433741	8000.024091	9.726490	-0.053051	4.815530
255.563072	8000.052931	9.731495	-0.053075	4.815538
255.729546	8000.075970	9.736499	-0.053106	4.815544
255.638332	8000.039248	9.741504	-0.053090	4.815533
255.585988	8000.124930	9.746509	-0.053080	4.815559
255.527607	8000.109040	9.751514	-0.053070	4.815554
255.529445	8000.111226	9.756519	-0.053070	4.815555
255.689894	8000.089305	9.761523	-0.053100	4.815548
255.607565	8000.066614	9.766528	-0.053085	4.815542
255.786797	8000.089862	9.771533	-0.053119	4.815547
255.628595	8000.075542	9.776538	-0.053089	4.815544
255.494939	8000.069101	9.781543	-0.053065	4.815543
255.653431	8000.089873	9.786547	-0.053095	4.815548
255.755528	8000.070202	9.791552	-0.053114	4.815542
255.705025	8000.108916	9.796557	-0.053105	4.815553
255.333206	8000.070804	9.801562	-0.053036	4.815544
255.654829	8000.063271	9.806567	-0.053096	4.815540
255.665080	8000.079480	9.811571	-0.053098	4.815545
255.457598	8000.028038	9.816576	-0.053059	4.815531
255.425990	8000.072401	9.821581	-0.053054	4.815544
255.822895	8000.053283	9.826586	-0.053128	4.815537
255.572742	8000.029981	9.831591	-0.053081	4.815531
255.643620	8000.045046	9.836595	-0.053095	4.815535
255.667355	8000.018751	9.841600	-0.053100	4.815527
255.839746	8000.087817	9.846605	-0.053132	4.815547
255.900556	8000.059993	9.851610	-0.053143	4.815538
255.755090	8000.082198	9.856615	-0.053117	4.815545
256.044726	8000.089096	9.861619	-0.053171	4.815546
255.668102	8000.076540	9.866624	-0.053101	4.815544
255.724314	8000.090298	9.871629	-0.053112	4.815548
255.779395	8000.090151	9.876634	-0.053122	4.815547
255.848982	8000.040039	9.881639	-0.053135	4.815532
255.823254	8000.066341	9.886643	-0.053131	4.815540
255.805747	8000.048983	9.891648	-0.053128	4.815535
256.039641	8000.076331	9.896653	-0.053171	4.815542
255.692817	8000.052515	9.901658	-0.053107	4.815537
255.766876	8000.064428	9.906663	-0.053121	4.815540
255.782565	8000.098885	9.911667	-0.053124	4.815550
256.099435	8000.079525	9.916672	-0.053183	4.815543
256.151856	8000.106038	9.921677	-0.053193	4.815550
256.078696	8000.105928	9.926682	-0.053180	4.815551
256.022284	8000.111433	9.931687	-0.053170	4.815552
255.915173	8000.133198	9.936691	-0.053150	4.815559
255.937740	8000.126110	9.941696	-0.053154	4.815557
256.254146	8000.141992	9.946701	-0.053214	4.815560
255.864948	8000.106799	9.951706	-0.053141	4.815552
255.775580	8000.126718	9.956711	-0.053125	4.815558
255.925011	8000.116366	9.961715	-0.053153	4.815554
255.790786	8000.003102	9.966720	-0.053128	4.815522
255.953570	8000.092306	9.971725	-0.053159	4.815547
255.909040	8000.086255	9.976730	-0.053151	4.815546
256.116092	8000.042667	9.981735	-0.053189	4.815532
256.120097	8000.084409	9.986739	-0.053190	4.815544
256.206271	8000.078363	9.991744	-0.053207	4.815542
256.218793	8000.111700	9.996749	-0.053209	4.815552
256.094415	8000.096865	10.001754	-0.053186	4.815548
255.997970	8000.132691	10.006759	-0.053169	4.815559
256.168946	8000.119488	10.011763	-0.053201	4.815554
256.250771	8000.120847	10.016768	-0.053216	4.815554
256.345248	8000.152323	10.021773	-0.053234	4.815563
256.233804	8000.102450	10.026778	-0.053213	4.815549
256.022456	8000.107554	10.031783	-0.053174	4.815551
256.128677	8000.122131	10.036787	-0.053194	4.815555
256.194570	8000.079435	10.041792	-0.053207	4.815542
256.395631	8000.123337	10.046797	-0.053244	4.815554
256.193883	8000.102962	10.051802	-0.053207	4.815549
255.968063	8000.103557	10.056807	-0.053165	4.815550
256.182256	8000.123106	10.061811	-0.053205	4.815555
256.149697	8000.049958	10.066816	-0.053199	4.815534
256.026693	8000.106711	10.071821	-0.053177	4.815551
256.089644	8000.088535	10.076826	-0.053189	4.815545
256.197456	8000.120228	10.081831	-0.053209	4.815554
256.120625	8000.128603	10.086835	-0.053195	4.815557
256.233796	8000.096295	10.091840	-0.053216	4.815547
256.261464	8000.121335	10.096845	-0.053222	4.815554
256.337885	8000.094834	10.101850	-0.053236	4.815546
256.033179	8000.081319	10.106855	-0.053179	4.815543
256.270852	8000.114070	10.111859	-0.053224	4.815552
256.036885	8000.032284	10.116864	-0.053181	4.815529
256.088066	8000.083344	10.121869	-0.053190	4.815544
256.336031	8000.057516	10.126874	-0.053237	4.815535
256.320882	8000.085059	10.131879	-0.053234	4.815543
256.230815	8000.117785	10.136883	-0.053218	4.815553
256.182269	8000.083897	10.141888	-0.053209	4.815543
256.427846	8000.089006	10.146893	-0.053255	4.815544
256.167442	8000.067671	10.151898	-0.053206	4.815539
256.216566	8000.078108	10.156903	-0.053216	4.815542
256.304434	8000.126565	10.161907	-0.053232	4.815555
256.206324	8000.084388	10.166912	-0.053214	4.815543
256.358719	8000.110403	10.171917	-0.053243	4.815550
256.405522	8000.072735	10.176922	-0.053252	4.815539
256.454701	8000.074628	10.181927	-0.053261	4.815539
256.283555	8000.098549	10.186931	-0.053230	4.815547
256.205690	8000.057772	10.191936	-0.053215	4.815536
256.378635	8000.103350	10.196941	-0.053248	4.815548
256.423129	8000.096621	10.201946	-0.053256	4.815546
256.286674	8000.066634	10.206951	-0.053231	4.815538
256.312404	8000.091642	10.211955	-0.053236	4.815545
256.231527	8000.095678	10.216960	-0.053221	4.815547
256.442296	8000.135467	10.221965	-0.053261	4.815557
256.343636	8000.130666	10.226970	-0.053243	4.815556
256.515615	8000.092912	10.231975	-0.053275	4.815544
256.379665	8000.098182	10.236979	-0.053250	4.815547
256.351919	8000.019772	10.241984	-0.053245	4.815524
256.594001	8000.117754	10.246989	-0.053290	4.815551
256.513031	8000.111107	10.251994	-0.053275	4.815550
256.407372	8000.099782	10.256999	-0.053256	4.815547
256.437754	8000.075732	10.262003	-0.053262	4.815540
256.391827	8000.049363	10.267008	-0.053253	4.815532
256.544511	8000.090337	10.272013	-0.053282	4.815543
256.429391	8000.072449	10.277018	-0.053261	4.815539
256.551102	8000.077666	10.282023	-0.053284	4.815540
256.510240	8000.124016	10.287027	-0.053276	4.815553
256.397870	8000.061310	10.292032	-0.053256	4.815536
256.351989	8000.111849	10.297037	-0.053247	4.815551
256.623883	8000.098163	10.302042	-0.053298	4.815545
256.230684	8000.105629	10.307047	-0.053225	4.815549
256.375348	8000.147540	10.312051	-0.053252	4.815561
256.438744	8000.099462	10.317056	-0.053264	4.815547
256.518772	8000.127497	10.322061	-0.053279	4.815554
256.522130	8000.077368	10.327066	-0.053280	4.815540
256.636218	8000.112369	10.332071	-0.053302	4.815549
256.733405	8000.140684	10.337075	-0.053320	4.815557
256.385500	8000.096552	10.342080	-0.053256	4.815546
256.496295	8000.144317	10.347085	-0.053276	4.815559
256.630599	8000.136923	10.352090	-0.053302	4.815557
256.566110	8000.092091	10.357095	-0.053290	4.815544
256.653395	8000.142676	10.362099	-0.053306	4.815558
256.331219	8000.127805	10.367104	-0.053247	4.815555
256.492724	8000.141152	10.372109	-0.053277	4.815558
256.361987	8000.131553	10.377114	-0.053253	4.815556
256.452842	8000.112765	10.382119	-0.053270	4.815550
256.504488	8000.128585	10.387123	-0.053280	4.815555
256.413199	8000.083315	10.392128	-0.053263	4.815542
256.512074	8000.093499	10.397133	-0.053282	4.815544
256.642034	8000.129828	10.402138	-0.053306	4.815554
256.466040	8000.041512	10.407143	-0.053273	4.815529
256.441685	8000.102018	10.412147	-0.053269	4.815547
256.850064	8000.090568	10.417152	-0.053345	4.815542
256.712865	8000.108635	10.422157	-0.053320	4.815548
256.572443	8000.104218	10.427162	-0.053294	4.815547
256.750825	8000.100751	10.432167	-0.053328	4.815545
256.728558	8000.133519	10.437171	-0.053324	4.815555
256.485576	8000.090036	10.442176	-0.053279	4.815543
256.652641	8000.101337	10.447181	-0.053310	4.815546
256.703729	8000.096853	10.452186	-0.053320	4.815544
256.683191	8000.084786	10.457191	-0.053316	4.815541
256.762804	8000.126700	10.462195	-0.053331	4.815553
256.777973	8000.077832	10.467200	-0.053334	4.815538
256.769437	8000.147143	10.472205	-0.053333	4.815559
256.543916	8000.144537	10.477210	-0.053291	4.815559
256.592909	8000.140018	10.482215	-0.053300	4.815557
256.858515	8000.141184	10.487219	-0.053350	4.815557
256.507429	8000.077772	10.492224	-0.053285	4.815540
256.772613	8000.124861	10.497229	-0.053335	4.815552
256.672310	8000.080511	10.502234	-0.053316	4.815540
256.753217	8000.111765	10.507239	-0.053331	4.815548
256.884659	8000.106460	10.512243	-0.053356	4.815546
256.954781	8000.112969	10.517248	-0.053369	4.815548
256.960238	8000.091714	10.522253	-0.053371	4.815542
256.887894	8000.127935	10.527258	-0.053357	4.815552
256.615896	8000.095727	10.532263	-0.053307	4.815544
256.813372	8000.101117	10.537267	-0.053344	4.815545
256.648146	8000.117658	10.542272	-0.053313	4.815551
256.635329	8000.137762	10.547277	-0.053311	4.815557
256.720046	8000.113534	10.552282	-0.053327	4.815549
256.706297	8000.100510	10.557287	-0.053325	4.815545
256.705995	8000.137910	10.562291	-0.053325	4.815556
256.700718	8000.106867	10.567296	-0.053324	4.815547
256.902397	8000.124076	10.572301	-0.053362	4.815551
256.601392	8000.123438	10.577306	-0.053306	4.815552
256.596456	8000.092399	10.582311	-0.053305	4.815543
256.760206	8000.145305	10.587315	-0.053336	4.815558
256.849493	8000.117947	10.592320	-0.053353	4.815550
256.705531	8000.107063	10.597325	-0.053326	4.815547
256.967178	8000.124186	10.602330	-0.053375	4.815551
256.982896	8000.045418	10.607335	-0.053379	4.815528
256.815230	8000.115327	10.612339	-0.053348	4.815549
256.791294	8000.048728	10.617344	-0.053343	4.815530
257.059965	8000.102285	10.622349	-0.053394	4.815544
256.836155	8000.120001	10.627354	-0.053352	4.815550
256.648381	8000.104127	10.632359	-0.053317	4.815547
256.909766	8000.158632	10.637363	-0.053366	4.815561
256.878996	8000.120762	10.642368	-0.053361	4.815550
256.856939	8000.146056	10.647373	-0.053357	4.815558
256.922780	8000.125791	10.652378	-0.053369	4.815552
257.052507	8000.123663	10.657383	-0.053394	4.815550
257.012920	8000.119829	10.662387	-0.053387	4.815549
256.994804	8000.119552	10.667392	-0.053383	4.815549
256.931195	8000.077939	10.672397	-0.053372	4.815537
257.158127	8000.080608	10.677402	-0.053414	4.815537
257.113290	8000.117279	10.682407	-0.053406	4.815548
257.220095	8000.152162	10.687411	-0.053426	4.815558
257.144555	8000.121035	10.692416	-0.053412	4.815549
256.716279	8000.142879	10.697421	-0.053333	4.815557
256.847686	8000.109802	10.702426	-0.053358	4.815547
257.003910	8000.119858	10.707431	-0.053387	4.815549
256.983904	8000.135572	10.712435	-0.053383	4.815554
256.970001	8000.099046	10.717440	-0.053381	4.815543
256.805976	8000.116674	10.722445	-0.053351	4.815549
256.771988	8000.107591	10.727450	-0.053345	4.815547
256.716036	8000.101353	10.732455	-0.053334	4.815545
257.051071	8000.138907	10.737459	-0.053397	4.815555
257.020699	8000.107451	10.742464	-0.053392	4.815546
256.979847	8000.143120	10.747469	-0.053384	4.815556
257.050467	8000.112251	10.752474	-0.053398	4.815547
257.130180	8000.102894	10.757479	-0.053413	4.815544
257.010589	8000.120182	10.762483	-0.053391	4.815549
256.889231	8000.065873	10.767488	-0.053368	4.815534
257.029751	8000.078876	10.772493	-0.053395	4.815537
257.054167	8000.067546	10.777498	-0.053399	4.815534
256.976812	8000.031048	10.782503	-0.053385	4.815523
257.038409	8000.055577	10.787507	-0.053397	4.815530
256.950059	8000.113967	10.792512	-0.053381	4.815548
256.857862	8000.118885	10.797517	-0.053364	4.815550
256.802800	8000.112662	10.802522	-0.053354	4.815548
256.917232	8000.071829	10.807527	-0.053375	4.815536
256.925275	8000.135003	10.812531	-0.053377	4.815554
256.674445	8000.110618	10.817536	-0.053330	4.815548
256.796519	8000.109433	10.822541	-0.053353	4.815547
257.018216	8000.118425	10.827546	-0.053395	4.815549
256.738584	8000.119204	10.832551	-0.053343	4.815550
256.976418	8000.143415	10.837555	-0.053388	4.815556
257.183138	8000.127594	10.842560	-0.053426	4.815551
257.070410	8000.130040	10.847565	-0.053406	4.815552
257.038405	8000.100694	10.852570	-0.053400	4.815543
257.043364	8000.094386	10.857575	-0.053401	4.815542
257.053271	8000.134090	10.862579	-0.053403	4.815553
256.826123	8000.095139	10.867584	-0.053361	4.815543
256.887854	8000.141033	10.872589	-0.053373	4.815556
256.903577	8000.128492	10.877594	-0.053376	4.815552
256.820870	8000.086566	10.882599	-0.053361	4.815540
256.909124	8000.137168	10.887603	-0.053377	4.815555
256.936115	8000.116266	10.892608	-0.053383	4.815548
257.136049	8000.130243	10.897613	-0.053420	4.815552
257.020050	8000.109134	10.902618	-0.053399	4.815546
257.044320	8000.072165	10.907623	-0.053403	4.815535
257.031129	8000.109355	10.912627	-0.053401	4.815546
256.926758	8000.089506	10.917632	-0.053382	4.815541
256.932945	8000.144104	10.922637	-0.053383	4.815557
256.932440	8000.127024	10.927642	-0.053383	4.815552
256.872854	8000.111113	10.932647	-0.053373	4.815547
256.913819	8000.079758	10.937651	-0.053380	4.815538
256.983626	8000.071308	10.942656	-0.053394	4.815535
257.075323	8000.126239	10.947661	-0.053411	4.815551
256.915276	8000.092659	10.952666	-0.053381	4.815542
256.977281	8000.083013	10.957671	-0.053393	4.815538
257.181317	8000.145125	10.962675	-0.053431	4.815556
256.872293	8000.085604	10.967680	-0.053374	4.815540
257.043422	8000.163200	10.972685	-0.053406	4.815562
257.009823	8000.140237	10.977690	-0.053400	4.815555
256.863054	8000.025694	10.982695	-0.053373	4.815522
256.915022	8000.121632	10.987699	-0.053383	4.815550
256.960096	8000.106368	10.992704	-0.053391	4.815545
257.293687	8000.115057	10.997709	-0.053454	4.815546
257.204338	8000.122158	11.002714	-0.053437	4.815549
257.295121	8000.093756	11.007719	-0.053454	4.815540
257.028637	8000.148160	11.012723	-0.053405	4.815557
257.015505	8000.115919	11.017728	-0.053403	4.815548
257.010491	8000.144697	11.022733	-0.053402	4.815556
257.019829	8000.129915	11.027738	-0.053404	4.815552
257.013991	8000.131975	11.032743	-0.053403	4.815552
256.934252	8000.140302	11.037747	-0.053389	4.815555
257.044276	8000.094056	11.042752	-0.053409	4.815541
257.021522	8000.056316	11.047757	-0.053405	4.815530
257.081649	8000.104321	11.052762	-0.053417	4.815544
256.961080	8000.056434	11.057767	-0.053394	4.815531
257.115324	8000.108116	11.062771	-0.053423	4.815545
257.123786	8000.096524	11.067776	-0.053425	4.815542
257.109970	8000.102727	11.072781	-0.053423	4.815543
257.168464	8000.130409	11.077786	-0.053434	4.815551
257.154210	8000.104559	11.082791	-0.053432	4.815544
256.999941	8000.156528	11.087795	-0.053403	4.815560
257.016999	8000.114100	11.092800	-0.053406	4.815547
257.164615	8000.128288	11.097805	-0.053434	4.815551
257.077455	8000.123675	11.102810	-0.053418	4.815550
257.026948	8000.096163	11.107815	-0.053409	4.815542
257.211289	8000.141930	11.112819	-0.053444	4.815554
257.000883	8000.079752	11.117824	-0.053405	4.815537
257.007186	8000.101238	11.122829	-0.053406	4.815543
257.130769	8000.118237	11.127834	-0.053429	4.815548
257.074487	8000.108789	11.132839	-0.053419	4.815545
257.236530	8000.147782	11.137843	-0.053449	4.815556
257.220592	8000.101608	11.142848	-0.053447	4.815542
257.332303	8000.112004	11.147853	-0.053468	4.815545
257.076084	8000.152689	11.152858	-0.053420	4.815558
257.161037	8000.128464	11.157863	-0.053436	4.815551
257.372356	8000.175742	11.162867	-0.053476	4.815563
257.292235	8000.098607	11.167872	-0.053461	4.815541
257.110748	8000.105267	11.172877	-0.053427	4.815544
257.239910	8000.129834	11.177882	-0.053452	4.815551
257.273487	8000.075927	11.182887	-0.053458	4.815535
257.107707	8000.108480	11.187891	-0.053428	4.815545
257.116008	8000.060568	11.192896	-0.053429	4.815531
257.294922	8000.107314	11.197901	-0.053463	4.815544
257.278243	8000.100651	11.202906	-0.053460	4.815542
257.069911	8000.082303	11.207911	-0.053421	4.815537
257.228911	8000.114836	11.212915	-0.053451	4.815546
257.151695	8000.091159	11.217920	-0.053437	4.815540
257.224717	8000.137239	11.222925	-0.053451	4.815553
257.149245	8000.131749	11.227930	-0.053437	4.815552
257.298878	8000.101106	11.232935	-0.053465	4.815542
257.264463	8000.139017	11.237939	-0.053459	4.815553
257.387769	8000.115420	11.242944	-0.053482	4.815546
257.342149	8000.143533	11.247949	-0.053474	4.815554
257.412908	8000.125485	11.252954	-0.053487	4.815548
257.147680	8000.105136	11.257959	-0.053438	4.815544
257.290435	8000.145949	11.262963	-0.053465	4.815555
257.174780	8000.116301	11.267968	-0.053444	4.815547
257.379498	8000.126084	11.272973	-0.053482	4.815549
257.123398	8000.125112	11.277978	-0.053434	4.815550
257.306922	8000.074729	11.282983	-0.053469	4.815534
257.475559	8000.130921	11.287987	-0.053501	4.815550
257.279709	8000.109572	11.292992	-0.053464	4.815544
257.290678	8000.159977	11.297997	-0.053467	4.815559
257.357979	8000.156826	11.303002	-0.053479	4.815558
257.135280	8000.126492	11.308007	-0.053438	4.815550
257.300451	8000.132423	11.313011	-0.053469	4.815551
257.367463	8000.106835	11.318016	-0.053482	4.815543
257.255821	8000.143480	11.323021	-0.053461	4.815554
257.210171	8000.127797	11.328026	-0.053453	4.815550
257.434798	8000.115475	11.333031	-0.053495	4.815545
257.400062	8000.148039	11.338035	-0.053489	4.815555
257.073227	8000.132021	11.343040	-0.053428	4.815552
257.204747	8000.149150	11.348045	-0.053453	4.815556
257.314729	8000.152040	11.353050	-0.053473	4.815557
257.369957	8000.140147	11.358055	-0.053484	4.815553
257.448671	8000.169229	11.363059	-0.053499	4.815561
257.541139	8000.123763	11.368064	-0.053516	4.815547
257.409867	8000.139791	11.373069	-0.053492	4.815552
257.188434	8000.152205	11.378074	-0.053451	4.815557
257.208347	8000.109823	11.383079	-0.053455	4.815545
257.318944	8000.154383	11.388083	-0.053476	4.815557
257.413758	8000.119637	11.393088	-0.053494	4.815547
257.237562	8000.141338	11.398093	-0.053461	4.815554
257.286128	8000.138949	11.403098	-0.053470	4.815553
257.113780	8000.116917	11.408103	-0.053438	4.815547
257.486490	8000.124112	11.413107	-0.053508	4.815547
257.414808	8000.098388	11.418112	-0.053495	4.815540
257.473146	8000.126069	11.423117	-0.053506	4.815548
257.366166	8000.125403	11.428122	-0.053486	4.815548
257.342754	8000.103676	11.433127	-0.053482	4.815542
257.531117	8000.122805	11.438131	-0.053518	4.815547
257.267832	8000.131328	11.443136	-0.053469	4.815551
257.334721	8000.126035	11.448141	-0.053481	4.815549
257.464485	8000.105748	11.453146	-0.053506	4.815542
257.265053	8000.127069	11.458151	-0.053469	4.815549
257.416546	8000.133843	11.463155	-0.053497	4.815551
257.383509	8000.145072	11.468160	-0.053491	4.815554
257.711606	8000.151536	11.473165	-0.053553	4.815554
257.486992	8000.167102	11.478170	-0.053511	4.815560
257.447296	8000.111993	11.483175	-0.053504	4.815544
257.514099	8000.176131	11.488179	-0.053517	4.815562
257.422541	8000.140468	11.493184	-0.053500	4.815552
257.443211	8000.144031	11.498189	-0.053504	4.815553
257.365456	8000.117140	11.503194	-0.053490	4.815546
257.399688	8000.100629	11.508199	-0.053496	4.815541
257.514195	8000.120684	11.513203	-0.053518	4.815546
257.421249	8000.114908	11.518208	-0.053501	4.815545
257.309135	8000.159023	11.523213	-0.053480	4.815558
257.297343	8000.148167	11.528218	-0.053478	4.815555
257.203421	8000.099647	11.533223	-0.053461	4.815542
257.243734	8000.141987	11.538227	-0.053468	4.815554
257.328732	8000.119899	11.543232	-0.053485	4.815547
257.484806	8000.105385	11.548237	-0.053514	4.815542
257.725552	8000.143532	11.553242	-0.053559	4.815552
257.234815	8000.121623	11.558247	-0.053468	4.815548
257.303803	8000.167637	11.563251	-0.053481	4.815561
257.584978	8000.122059	11.568256	-0.053533	4.815546
257.636242	8000.127192	11.573261	-0.053543	4.815547
257.686012	8000.132300	11.578266	-0.053553	4.815549
257.509364	8000.103788	11.583271	-0.053520	4.815541
257.710302	8000.138078	11.588275	-0.053558	4.815550
257.515559	8000.129565	11.593280	-0.053522	4.815549
257.437164	8000.120822	11.598285	-0.053507	4.815547
257.600415	8000.136336	11.603290	-0.053538	4.815550
257.407772	8000.126789	11.608295	-0.053502	4.815548
257.419797	8000.160120	11.613299	-0.053505	4.815558
257.335619	8000.149146	11.618304	-0.053489	4.815555
257.483524	8000.148385	11.623309	-0.053517	4.815554
257.417658	8000.167621	11.628314	-0.053505	4.815560
257.375126	8000.137034	11.633319	-0.053497	4.815552
257.631040	8000.152997	11.638323	-0.053545	4.815555
257.499659	8000.132705	11.643328	-0.053521	4.815550
257.682877	8000.095135	11.648333	-0.053555	4.815538
257.629462	8000.134871	11.653338	-0.053545	4.815550
257.602397	8000.116287	11.658343	-0.053541	4.815544
257.555577	8000.150790	11.663347	-0.053532	4.815555
257.350988	8000.103661	11.668352	-0.053494	4.815542
257.454582	8000.105378	11.673357	-0.053514	4.815542
257.649625	8000.147049	11.678362	-0.053550	4.815553
257.454414	8000.062687	11.683367	-0.053514	4.815529
257.553487	8000.098512	11.688371	-0.053533	4.815539
257.795431	8000.123861	11.693376	-0.053578	4.815546
257.569319	8000.155425	11.698381	-0.053536	4.815556
257.448908	8000.152403	11.703386	-0.053514	4.815556
257.391837	8000.106623	11.708391	-0.053504	4.815542
257.322041	8000.125795	11.713395	-0.053491	4.815548
257.519278	8000.124774	11.718400	-0.053528	4.815547
257.533649	8000.131438	11.723405	-0.053531	4.815549
257.524410	8000.132374	11.728410	-0.053529	4.815549
257.419657	8000.124268	11.733415	-0.053510	4.815547
257.552262	8000.153166	11.738419	-0.053535	4.815555
257.566854	8000.149152	11.743424	-0.053538	4.815554
257.504091	8000.097937	11.748429	-0.053526	4.815539
257.569333	8000.121458	11.753434	-0.053539	4.815546
257.713700	8000.113162	11.758439	-0.053566	4.815543
257.439136	8000.140728	11.763443	-0.053515	4.815552
257.741717	8000.101910	11.768448	-0.053571	4.815539
257.924470	8000.136971	11.773453	-0.053606	4.815549
257.623413	8000.151284	11.778458	-0.053550	4.815554
257.715788	8000.110089	11.783463	-0.053567	4.815542
257.708539	8000.140968	11.788467	-0.053566	4.815551
257.749235	8000.119222	11.793472	-0.053574	4.815544
257.577392	8000.139926	11.798477	-0.053542	4.815551
257.605606	8000.143612	11.803482	-0.053548	4.815552
257.552397	8000.102168	11.808487	-0.053538	4.815540
257.700185	8000.156952	11.813491	-0.053566	4.815556
257.514080	8000.128284	11.818496	-0.053531	4.815548
257.618845	8000.117202	11.823501	-0.053551	4.815544
257.590879	8000.116764	11.828506	-0.053546	4.815544
257.537224	8000.075312	11.833511	-0.053536	4.815532
257.745658	8000.116135	11.838515	-0.053575	4.815543
257.827352	8000.117493	11.843520	-0.053591	4.815543
257.736887	8000.113894	11.848525	-0.053574	4.815543
257.666991	8000.131995	11.853530	-0.053561	4.815548
257.641206	8000.069637	11.858535	-0.053557	4.815530
257.742282	8000.124723	11.863539	-0.053576	4.815546
257.670237	8000.135312	11.868544	-0.053563	4.815549
257.472190	8000.127813	11.873549	-0.053526	4.815548
257.524969	8000.141516	11.878554	-0.053536	4.815552
257.539142	8000.092630	11.883559	-0.053539	4.815537
257.556313	8000.145273	11.888563	-0.053542	4.815553
257.675012	8000.120533	11.893568	-0.053565	4.815545
257.505167	8000.071837	11.898573	-0.053533	4.815532
257.586022	8000.110568	11.903578	-0.053548	4.815542
257.770340	8000.117881	11.908583	-0.053583	4.815544
257.630992	8000.158345	11.913587	-0.053557	4.815556
257.526205	8000.137420	11.918592	-0.053538	4.815551
257.584857	8000.112764	11.923597	-0.053549	4.815543
257.700000	8000.153125	11.928602	-0.053571	4.815554
257.552464	8000.130431	11.933607	-0.053544	4.815548
257.851894	8000.160995	11.938611	-0.053599	4.815556
257.668382	8000.124893	11.943616	-0.053566	4.815546
257.524588	8000.125760	11.948621	-0.053539	4.815547
257.585092	8000.125703	11.953626	-0.053550	4.815547
257.548125	8000.077048	11.958631	-0.053544	4.815533
257.624067	8000.112494	11.963635	-0.053558	4.815543
257.680607	8000.129464	11.968640	-0.053569	4.815547
257.811704	8000.065403	11.973645	-0.053594	4.815528
257.715701	8000.094827	11.978650	-0.053576	4.815537
257.644394	8000.081928	11.983655	-0.053563	4.815534
257.682945	8000.103943	11.988659	-0.053570	4.815540
257.870275	8000.126261	11.993664	-0.053605	4.815546
257.799028	8000.148613	11.998669	-0.053592	4.815552
257.593279	8000.170897	12.003674	-0.053554	4.815560
257.674145	8000.109218	12.008679	-0.053569	4.815542
257.861475	8000.139013	12.013683	-0.053605	4.815549
257.633897	8000.103257	12.018688	-0.053562	4.815540
257.733928	8000.082483	12.023693	-0.053581	4.815533
257.773269	8000.133353	12.028698	-0.053589	4.815548
257.544451	8000.084758	12.033703	-0.053546	4.815535
257.544504	8000.132848	12.038707	-0.053547	4.815549
257.741303	8000.122206	12.043712	-0.053584	4.815545
257.720095	8000.136833	12.048717	-0.053580	4.815549
257.675643	8000.145738	12.053722	-0.053572	4.815552
257.891962	8000.089483	12.058727	-0.053612	4.815535
257.751851	8000.160913	12.063731	-0.053586	4.815556
257.583810	8000.143223	12.068736	-0.053555	4.815552
257.710963	8000.083371	12.073741	-0.053579	4.815534
257.841648	8000.129329	12.078746	-0.053604	4.815547
257.548034	8000.105309	12.083751	-0.053549	4.815541
257.816493	8000.137501	12.088755	-0.053600	4.815549
257.897838	8000.118558	12.093760	-0.053615	4.815543
257.556778	8000.117261	12.098765	-0.053552	4.815544
257.539399	8000.138359	12.103770	-0.053549	4.815551
257.650624	8000.108156	12.108775	-0.053570	4.815541
257.710469	8000.139066	12.113779	-0.053581	4.815550
257.703861	8000.084499	12.118784	-0.053580	4.815534
257.643609	8000.101690	12.123789	-0.053569	4.815539
257.926007	8000.118088	12.128794	-0.053622	4.815543
257.655926	8000.069885	12.133799	-0.053572	4.815530
257.598941	8000.096744	12.138803	-0.053561	4.815538
257.629921	8000.073771	12.143808	-0.053567	4.815531
257.680620	8000.075690	12.148813	-0.053577	4.815532
257.678297	8000.144036	12.153818	-0.053577	4.815552
257.811074	8000.138754	12.158823	-0.053602	4.815549
257.860029	8000.159872	12.163827	-0.053611	4.815555
257.808770	8000.137687	12.168832	-0.053602	4.815549
257.690162	8000.135763	12.173837	-0.053580	4.815549
257.871872	8000.169739	12.178842	-0.053614	4.815558
257.848149	8000.124505	12.183847	-0.053610	4.815545
257.753257	8000.165697	12.188851	-0.053592	4.815557
257.650469	8000.150146	12.193856	-0.053573	4.815553
257.768093	8000.125388	12.198861	-0.053595	4.815546
257.807007	8000.148478	12.203866	-0.053603	4.815552
257.566719	8000.106104	12.208871	-0.053558	4.815541
257.645509	8000.106346	12.213875	-0.053573	4.815541
257.720739	8000.097985	12.218880	-0.053587	4.815538
257.616671	8000.118731	12.223885	-0.053568	4.815544
257.816733	8000.126302	12.228890	-0.053606	4.815546
257.589420	8000.126869	12.233895	-0.053564	4.815547
257.573223	8000.131964	12.238899	-0.053561	4.815548
257.657129	8000.115200	12.243904	-0.053577	4.815543
257.564377	8000.091267	12.248909	-0.053560	4.815537
257.724456	8000.137706	12.253914	-0.053590	4.815549
257.579891	8000.096901	12.258919	-0.053563	4.815538
257.969169	8000.086209	12.263923	-0.053636	4.815533
257.992907	8000.096232	12.268928	-0.053640	4.815536
257.559863	8000.058176	12.273933	-0.053560	4.815527
257.746108	8000.098635	12.278938	-0.053595	4.815538
257.748968	8000.085883	12.283943	-0.053596	4.815534
257.619579	8000.125442	12.288947	-0.053572	4.815546
257.757588	8000.122383	12.293952	-0.053598	4.815545
257.526195	8000.031018	12.298957	-0.053555	4.815519
257.770104	8000.123695	12.303962	-0.053600	4.815545
257.684272	8000.083853	12.308967	-0.053585	4.815534
257.949624	8000.120267	12.313971	-0.053634	4.815543
257.874750	8000.153242	12.318976	-0.053621	4.815553
257.828955	8000.164262	12.323981	-0.053612	4.815557
257.840932	8000.159137	12.328986	-0.053615	4.815555
257.763060	8000.090583	12.333991	-0.053600	4.815535
257.844267	8000.148548	12.338995	-0.053616	4.815552
257.665437	8000.122136	12.344000	-0.053583	4.815545
257.679393	8000.052951	12.349005	-0.053586	4.815525
257.879687	8000.113936	12.354010	-0.053623	4.815542
257.585594	8000.099522	12.359015	-0.053569	4.815539
257.816501	8000.134304	12.364019	-0.053612	4.815548
257.807554	8000.126700	12.369024	-0.053610	4.815546
257.869199	8000.092479	12.374029	-0.053622	4.815535
257.905808	8000.145441	12.379034	-0.053629	4.815551
257.883272	8000.135477	12.384039	-0.053625	4.815548
257.860309	8000.127642	12.389043	-0.053621	4.815546
257.695318	8000.129231	12.394048	-0.053591	4.815547
257.828814	8000.098324	12.399053	-0.053616	4.815537
257.996478	8000.125660	12.404058	-0.053647	4.815544
257.783637	8000.115782	12.409063	-0.053608	4.815542
257.823587	8000.134616	12.414067	-0.053615	4.815548
257.966963	8000.087848	12.419072	-0.053642	4.815533
257.808450	8000.079928	12.424077	-0.053613	4.815532
257.845475	8000.074145	12.429082	-0.053620	4.815530
257.750186	8000.093967	12.434087	-0.053603	4.815536
258.012974	8000.076930	12.439091	-0.053652	4.815530
257.806196	8000.101334	12.444096	-0.053613	4.815538
257.736120	8000.088454	12.449101	-0.053601	4.815535
258.076084	8000.125024	12.454106	-0.053664	4.815544
257.823102	8000.086715	12.459111	-0.053617	4.815534
258.063133	8000.112033	12.464115	-0.053662	4.815540
258.007963	8000.099398	12.469120	-0.053652	4.815537
257.975592	8000.137342	12.474125	-0.053646	4.815548
258.015846	8000.159386	12.479130	-0.053654	4.815554
258.013477	8000.120911	12.484135	-0.053654	4.815543
257.821156	8000.139142	12.489139	-0.053618	4.815549
257.977847	8000.135321	12.494144	-0.053648	4.815547
258.011252	8000.123069	12.499149	-0.053654	4.815543
258.082142	8000.134933	12.504154	-0.053667	4.815547
257.893873	8000.117980	12.509159	-0.053633	4.815542
257.855439	8000.151552	12.514163	-0.053626	4.815552
258.005637	8000.176466	12.519168	-0.053654	4.815559
258.092039	8000.150129	12.524173	-0.053670	4.815551
258.069042	8000.181818	12.529178	-0.053666	4.815560
257.869427	8000.113404	12.534183	-0.053629	4.815541
257.969552	8000.148180	12.539187	-0.053648	4.815551
257.824785	8000.142621	12.544192	-0.053621	4.815550
257.817416	8000.117951	12.549197	-0.053620	4.815543
257.752018	8000.108353	12.554202	-0.053608	4.815540
257.779541	8000.092801	12.559207	-0.053614	4.815536
257.835576	8000.141808	12.564211	-0.053624	4.815550
257.866059	8000.118827	12.569216	-0.053630	4.815543
257.850438	8000.049157	12.574221	-0.053627	4.815523
257.859874	8000.088855	12.579226	-0.053629	4.815534
257.964018	8000.105536	12.584231	-0.053649	4.815538
258.056684	8000.138053	12.589235	-0.053666	4.815547
257.858625	8000.126280	12.594240	-0.053630	4.815545
257.828458	8000.088418	12.599245	-0.053624	4.815534
257.990048	8000.099632	12.604250	-0.053655	4.815537
257.862193	8000.097556	12.609255	-0.053631	4.815537
257.847120	8000.141125	12.614259	-0.053629	4.815549
257.919903	8000.143406	12.619264	-0.053642	4.815550
257.913331	8000.130499	12.624269	-0.053641	4.815546
257.908766	8000.143262	12.629274	-0.053641	4.815550
258.004209	8000.153392	12.634279	-0.053659	4.815552
257.820316	8000.136511	12.639283	-0.053625	4.815548
257.924089	8000.116867	12.644288	-0.053644	4.815542
257.814587	8000.118296	12.649293	-0.053624	4.815543
257.930236	8000.149053	12.654298	-0.053646	4.815551
257.814274	8000.147172	12.659303	-0.053624	4.815551
257.777154	8000.142310	12.664307	-0.053618	4.815550
257.847373	8000.113571	12.669312	-0.053631	4.815541
258.031268	8000.099513	12.674317	-0.053666	4.815536
258.164064	8000.156189	12.679322	-0.053691	4.815552
257.991161	8000.105304	12.684327	-0.053658	4.815538
257.994223	8000.117124	12.689331	-0.053659	4.815542
257.854307	8000.140488	12.694336	-0.053633	4.815549
257.786846	8000.031512	12.699341	-0.053621	4.815518
257.989206	8000.123510	12.704346	-0.053659	4.815543
258.074002	8000.106760	12.709351	-0.053675	4.815538
257.879495	8000.120683	12.714355	-0.053639	4.815543
258.067821	8000.120585	12.719360	-0.053674	4.815542
257.888482	8000.067458	12.724365	-0.053641	4.815528
257.876020	8000.128162	12.729370	-0.053639	4.815545
257.859988	8000.123646	12.734375	-0.053636	4.815544
258.195484	8000.119551	12.739379	-0.053699	4.815541
258.089571	8000.135994	12.744384	-0.053680	4.815547
257.735851	8000.121670	12.749389	-0.053614	4.815544
258.035206	8000.151165	12.754394	-0.053670	4.815551
258.047182	8000.086220	12.759399	-0.053672	4.815532
257.928624	8000.100319	12.764403	-0.053650	4.815537
258.051723	8000.120516	12.769408	-0.053674	4.815542
257.938437	8000.057791	12.774413	-0.053653	4.815524
258.123313	8000.107842	12.779418	-0.053687	4.815538
258.093015	8000.099888	12.784423	-0.053682	4.815536
258.130312	8000.105860	12.789427	-0.053689	4.815537
258.161251	8000.146979	12.794432	-0.053695	4.815549
257.844446	8000.102281	12.799437	-0.053636	4.815538
258.047188	8000.152625	12.804442	-0.053674	4.815552
258.229997	8000.119322	12.809447	-0.053709	4.815541
257.809531	8000.102836	12.814451	-0.053630	4.815538
257.979246	8000.105637	12.819456	-0.053662	4.815538
258.254189	8000.051412	12.824461	-0.053714	4.815521
258.097675	8000.086253	12.829466	-0.053685	4.815532
258.107713	8000.125961	12.834471	-0.053687	4.815543
258.225914	8000.071303	12.839475	-0.053709	4.815527
258.085619	8000.097865	12.844480	-0.053683	4.815535
258.065223	8000.067640	12.849485	-0.053680	4.815527
258.159469	8000.135434	12.854490	-0.053697	4.815546
258.082114	8000.091456	12.859495	-0.053683	4.815533
257.937074	8000.104054	12.864499	-0.053656	4.815538
257.993929	8000.128506	12.869504	-0.053667	4.815545
258.057850	8000.102868	12.874509	-0.053679	4.815537
258.041459	8000.118642	12.879514	-0.053677	4.815542
257.842439	8000.149582	12.884519	-0.053640	4.815552
258.111357	8000.147601	12.889523	-0.053690	4.815550
258.168044	8000.160300	12.894528	-0.053701	4.815553
258.117862	8000.099676	12.899533	-0.053692	4.815536
258.157544	8000.135598	12.904538	-0.053699	4.815546
257.967037	8000.129290	12.909543	-0.053664	4.815545
257.884476	8000.075614	12.914547	-0.053649	4.815530
257.921347	8000.113625	12.919552	-0.053656	4.815541
257.985590	8000.100811	12.924557	-0.053668	4.815537
258.102948	8000.107027	12.929562	-0.053690	4.815538
257.868544	8000.112818	12.934567	-0.053647	4.815541
258.206027	8000.094869	12.939571	-0.053710	4.815534
258.064332	8000.132090	12.944576	-0.053684	4.815545
257.971154	8000.087853	12.949581	-0.053667	4.815533
257.855129	8000.141518	12.954586	-0.053645	4.815549
257.976762	8000.116826	12.959591	-0.053668	4.815541
257.967949	8000.138066	12.964595	-0.053667	4.815547
257.928314	8000.110730	12.969600	-0.053659	4.815540
257.911900	8000.110481	12.974605	-0.053657	4.815540
258.285513	8000.166831	12.979610	-0.053726	4.815554
258.160311	8000.147707	12.984615	-0.053703	4.815549
258.146637	8000.135752	12.989619	-0.053701	4.815546
258.116309	8000.151297	12.994624	-0.053696	4.815551
258.005845	8000.083276	12.999629	-0.053675	4.815531
258.092254	8000.092190	13.004634	-0.053692	4.815533
258.056185	8000.101232	13.009639	-0.053685	4.815536
258.174831	8000.069014	13.014643	-0.053707	4.815526
258.245316	8000.091553	13.019648	-0.053721	4.815532
258.130870	8000.105720	13.024653	-0.053700	4.815537
258.356444	8000.152167	13.029658	-0.053742	4.815550
257.960689	8000.118993	13.034663	-0.053668	4.815542
258.037604	8000.160865	13.039667	-0.053683	4.815554
258.038255	8000.150213	13.044672	-0.053683	4.815551
258.063060	8000.117525	13.049677	-0.053688	4.815541
258.136936	8000.144393	13.054682	-0.053702	4.815548
258.063825	8000.107962	13.059687	-0.053689	4.815538
258.144935	8000.111448	13.064691	-0.053704	4.815539
258.121388	8000.150606	13.069696	-0.053700	4.815550
257.996168	8000.099434	13.074701	-0.053677	4.815536
258.104013	8000.158906	13.079706	-0.053697	4.815553
257.959617	8000.099943	13.084711	-0.053670	4.815536
258.121619	8000.083390	13.089715	-0.053701	4.815531
258.077972	8000.146787	13.094720	-0.053693	4.815549
257.988589	8000.118636	13.099725	-0.053676	4.815542
258.018237	8000.154393	13.104730	-0.053682	4.815552
257.969754	8000.102343	13.109735	-0.053673	4.815537
258.106072	8000.111007	13.114739	-0.053699	4.815539
257.892654	8000.131028	13.119744	-0.053660	4.815546
258.012546	8000.109512	13.124749	-0.053682	4.815539
258.074806	8000.079574	13.129754	-0.053694	4.815530
258.117395	8000.100588	13.134759	-0.053702	4.815536
258.061188	8000.054821	13.139763	-0.053692	4.815523
258.170010	8000.082262	13.144768	-0.053712	4.815530
257.944366	8000.107424	13.149773	-0.053670	4.815538
258.071729	8000.152261	13.154778	-0.053694	4.815551
258.113064	8000.097410	13.159783	-0.053702	4.815535
258.257880	8000.073098	13.164787	-0.053729	4.815527
258.195312	8000.130844	13.169792	-0.053718	4.815544
258.086573	8000.093830	13.174797	-0.053698	4.815534
258.328681	8000.176868	13.179802	-0.053743	4.815557
258.224864	8000.118569	13.184807	-0.053724	4.815540
258.160165	8000.088686	13.189811	-0.053712	4.815532
258.277191	8000.115193	13.194816	-0.053734	4.815539
258.176375	8000.097537	13.199821	-0.053716	4.815534
257.983967	8000.117903	13.204826	-0.053680	4.815541
258.001374	8000.073343	13.209831	-0.053684	4.815528
258.076162	8000.071383	13.214835	-0.053698	4.815527
258.229897	8000.103833	13.219840	-0.053727	4.815536
258.370739	8000.099753	13.224845	-0.053753	4.815534
258.104928	8000.111438	13.229850	-0.053704	4.815539
258.024475	8000.121889	13.234855	-0.053689	4.815542
258.101187	8000.101802	13.239859	-0.053704	4.815536
258.156044	8000.135835	13.244864	-0.053714	4.815546
258.152897	8000.125121	13.249869	-0.053714	4.815542
258.378037	8000.130968	13.254874	-0.053756	4.815543
258.316056	8000.095788	13.259879	-0.053745	4.815533
258.356687	8000.069768	13.264883	-0.053752	4.815525
258.082321	8000.137929	13.269888	-0.053701	4.815547
258.010853	8000.118617	13.274893	-0.053688	4.815541
258.415438	8000.150907	13.279898	-0.053764	4.815549
258.243695	8000.112860	13.284903	-0.053732	4.815538
258.164787	8000.041083	13.289907	-0.053718	4.815518
258.278636	8000.107062	13.294912	-0.053739	4.815537
258.243035	8000.109703	13.299917	-0.053733	4.815537
258.260333	8000.118552	13.304922	-0.053736	4.815540
258.346801	8000.110375	13.309927	-0.053752	4.815537
258.338658	8000.112397	13.314931	-0.053751	4.815538
258.137995	8000.133696	13.319936	-0.053714	4.815545
258.045180	8000.112966	13.324941	-0.053697	4.815539
258.202515	8000.119838	13.329946	-0.053727	4.815541
258.302008	8000.110807	13.334951	-0.053745	4.815537
258.157084	8000.120201	13.339955	-0.053719	4.815541
258.169075	8000.163146	13.344960	-0.053721	4.815553
258.149398	8000.122250	13.349965	-0.053718	4.815542
258.072724	8000.145582	13.354970	-0.053703	4.815549
258.062919	8000.098439	13.359975	-0.053702	4.815535
258.210943	8000.108363	13.364979	-0.053730	4.815537
258.253574	8000.155015	13.369984	-0.053738	4.815551
257.800418	8000.121968	13.374989	-0.053654	4.815543
258.275992	8000.149012	13.379994	-0.053742	4.815549
258.162511	8000.126875	13.384999	-0.053722	4.815543
258.133752	8000.106127	13.390003	-0.053716	4.815537
258.202601	8000.139322	13.395008	-0.053729	4.815546
258.223088	8000.127927	13.400013	-0.053733	4.815543
258.221632	8000.105490	13.405018	-0.053733	4.815536
258.112624	8000.115473	13.410023	-0.053713	4.815540
258.315763	8000.134846	13.415027	-0.053751	4.815544
258.507064	8000.160435	13.420032	-0.053787	4.815551
258.006140	8000.114854	13.425037	-0.053694	4.815540
258.138939	8000.125596	13.430042	-0.053719	4.815542
258.254086	8000.105071	13.435047	-0.053741	4.815536
257.837003	8000.139914	13.440051	-0.053663	4.815548
257.953434	8000.134364	13.445056	-0.053685	4.815546
257.972461	8000.120809	13.450061	-0.053689	4.815542
258.195988	8000.108470	13.455066	-0.053731	4.815537
258.194854	8000.098857	13.460071	-0.053731	4.815534
258.227649	8000.066299	13.465075	-0.053737	4.815525
258.290126	8000.109004	13.470080	-0.053749	4.815537
258.147881	8000.123783	13.475085	-0.053723	4.815542
258.130165	8000.151286	13.480090	-0.053720	4.815550
258.255462	8000.105289	13.485095	-0.053743	4.815536
258.186460	8000.069994	13.490099	-0.053731	4.815526
258.304084	8000.172356	13.495104	-0.053753	4.815555
258.254277	8000.079691	13.500109	-0.053744	4.815528
258.375262	8000.075285	13.505114	-0.053766	4.815527
258.167847	8000.071904	13.510119	-0.053728	4.815527
258.173600	8000.070950	13.515123	-0.053729	4.815526
258.482585	8000.118764	13.520128	-0.053787	4.815539
258.078158	8000.107880	13.525133	-0.053712	4.815537
258.105658	8000.158557	13.530138	-0.053717	4.815552
258.303999	8000.156487	13.535143	-0.053755	4.815551
258.222355	8000.117780	13.540147	-0.053740	4.815540
258.379653	8000.120379	13.545152	-0.053769	4.815540
258.356368	8000.084765	13.550157	-0.053765	4.815529
258.412725	8000.169031	13.555162	-0.053776	4.815554
258.080198	8000.132620	13.560167	-0.053714	4.815545
258.136761	8000.083360	13.565171	-0.053725	4.815530
258.543023	8000.138111	13.570176	-0.053801	4.815544
258.152425	8000.135999	13.575181	-0.053728	4.815545
258.226050	8000.174614	13.580186	-0.053742	4.815556
258.459928	8000.161376	13.585191	-0.053786	4.815551
258.185389	8000.144076	13.590195	-0.053735	4.815547
258.238656	8000.168470	13.595200	-0.053745	4.815554
258.399658	8000.130536	13.600205	-0.053775	4.815542
258.431368	8000.168464	13.605210	-0.053781	4.815553
258.197049	8000.134731	13.610215	-0.053738	4.815545
258.242266	8000.131219	13.615219	-0.053747	4.815543
258.356859	8000.164096	13.620224	-0.053768	4.815552
258.105358	8000.136491	13.625229	-0.053722	4.815546
258.197299	8000.166860	13.630234	-0.053739	4.815554
258.413794	8000.157611	13.635239	-0.053779	4.815550
258.241647	8000.160149	13.640243	-0.053748	4.815552
258.247108	8000.160258	13.645248	-0.053749	4.815552
258.257553	8000.128402	13.650253	-0.053751	4.815542
258.371076	8000.167671	13.655258	-0.053772	4.815553
258.282674	8000.158763	13.660263	-0.053756	4.815551
258.210367	8000.169348	13.665267	-0.053743	4.815555
258.440485	8000.205188	13.670272	-0.053786	4.815564
258.398144	8000.172466	13.675277	-0.053778	4.815555
258.246502	8000.162521	13.680282	-0.053750	4.815552
258.444345	8000.145489	13.685287	-0.053787	4.815547
258.383752	8000.155197	13.690291	-0.053776	4.815550
258.219794	8000.161074	13.695296	-0.053746	4.815552
258.118847	8000.113505	13.700301	-0.053727	4.815539
258.290216	8000.190042	13.705306	-0.053760	4.815560
258.175059	8000.145444	13.710311	-0.053738	4.815548
258.283364	8000.066054	13.715315	-0.053759	4.815524
258.397924	8000.160888	13.720320	-0.053780	4.815551
258.100168	8000.107955	13.725325	-0.053725	4.815537
258.314784	8000.156359	13.730330	-0.053765	4.815550
258.259169	8000.158671	13.735335	-0.053755	4.815551
258.160673	8000.159212	13.740339	-0.053737	4.815552
258.159843	8000.160287	13.745344	-0.053737	4.815552
258.194124	8000.152322	13.750349	-0.053744	4.815550
258.272636	8000.171789	13.755354	-0.053758	4.815555
258.277382	8000.151590	13.760359	-0.053760	4.815549
258.156177	8000.120780	13.765363	-0.053737	4.815541
258.297753	8000.176533	13.770368	-0.053764	4.815556
258.226068	8000.144398	13.775373	-0.053751	4.815547
258.275038	8000.153767	13.780378	-0.053760	4.815550
258.355777	8000.143359	13.785383	-0.053775	4.815546
258.397124	8000.160080	13.790387	-0.053783	4.815551
258.298830	8000.170239	13.795392	-0.053765	4.815554
258.282311	8000.147555	13.800397	-0.053762	4.815548
258.477456	8000.160388	13.805402	-0.053799	4.815551
258.450230	8000.135392	13.810407	-0.053794	4.815543
258.302002	8000.138322	13.815411	-0.053767	4.815545
258.431905	8000.198156	13.820416	-0.053791	4.815562
258.437684	8000.159814	13.825421	-0.053792	4.815551
258.282682	8000.196817	13.830426	-0.053764	4.815562
258.335798	8000.189161	13.835431	-0.053774	4.815560
258.111198	8000.118200	13.840435	-0.053732	4.815540
258.213995	8000.175453	13.845440	-0.053752	4.815556
258.102611	8000.153350	13.850445	-0.053731	4.815550
258.352087	8000.182029	13.855450	-0.053778	4.815557
258.247926	8000.169658	13.860455	-0.053759	4.815554
258.360213	8000.157632	13.865459	-0.053780	4.815550
258.437015	8000.156775	13.870464	-0.053794	4.815550
258.269566	8000.157253	13.875469	-0.053763	4.815551
258.228074	8000.181162	13.880474	-0.053756	4.815558
258.289319	8000.186459	13.885479	-0.053767	4.815559
258.435947	8000.168586	13.890483	-0.053795	4.815553
258.397345	8000.197883	13.895488	-0.053788	4.815562
258.329806	8000.156202	13.900493	-0.053776	4.815550
258.440687	8000.201838	13.905498	-0.053796	4.815563
258.276089	8000.188476	13.910503	-0.053766	4.815560
258.250911	8000.177400	13.915507	-0.053762	4.815557
258.251510	8000.189180	13.920512	-0.053762	4.815560
258.528673	8000.152084	13.925517	-0.053814	4.815548
258.374259	8000.215802	13.930522	-0.053785	4.815567
258.129154	8000.164800	13.935527	-0.053740	4.815553
258.218871	8000.186587	13.940531	-0.053757	4.815559
258.358793	8000.198515	13.945536	-0.053783	4.815562
258.247603	8000.150777	13.950541	-0.053762	4.815549
258.537067	8000.161953	13.955546	-0.053817	4.815551
258.416532	8000.171746	13.960551	-0.053794	4.815554
258.075873	8000.168317	13.965555	-0.053731	4.815555
258.373095	8000.208461	13.970560	-0.053787	4.815565
258.452098	8000.177729	13.975565	-0.053802	4.815556
258.450980	8000.201232	13.980570	-0.053802	4.815562
258.503310	8000.186086	13.985575	-0.053812	4.815558
258.494112	8000.152839	13.990579	-0.053810	4.815548
258.581483	8000.193817	13.995584	-0.053827	4.815560
258.392814	8000.178992	14.000589	-0.053792	4.815556
258.389210	8000.201385	14.005594	-0.053791	4.815563
258.370008	8000.151951	14.010599	-0.053788	4.815548
258.283181	8000.156956	14.015603	-0.053772	4.815550
258.343895	8000.186814	14.020608	-0.053784	4.815559
258.312441	8000.142520	14.025613	-0.053778	4.815546
258.489476	8000.179626	14.030618	-0.053811	4.815556
258.370210	8000.141370	14.035623	-0.053789	4.815545
258.352647	8000.154988	14.040627	-0.053786	4.815549
258.485054	8000.188158	14.045632	-0.053811	4.815558
258.490773	8000.129518	14.050637	-0.053812	4.815541
258.459075	8000.184566	14.055642	-0.053807	4.815557
258.602485	8000.188006	14.060647	-0.053833	4.815558
258.597781	8000.128127	14.065651	-0.053833	4.815540
258.736707	8000.177428	14.070656	-0.053859	4.815554
258.614672	8000.136989	14.075661	-0.053836	4.815543
258.690950	8000.166034	14.080666	-0.053851	4.815551
258.538754	8000.112282	14.085671	-0.053823	4.815536
258.610246	8000.146589	14.090675	-0.053836	4.815546
258.663692	8000.157100	14.095680	-0.053846	4.815548
258.756942	8000.120192	14.100685	-0.053864	4.815537
258.461397	8000.123911	14.105690	-0.053809	4.815540
258.367325	8000.162981	14.110695	-0.053792	4.815552
258.348052	8000.141319	14.115699	-0.053789	4.815545
258.454034	8000.142009	14.120704	-0.053808	4.815545
258.514239	8000.115241	14.125709	-0.053820	4.815537
258.486830	8000.120153	14.130714	-0.053815	4.815538
258.585461	8000.147427	14.135719	-0.053834	4.815546
258.575799	8000.112036	14.140723	-0.053832	4.815536
258.775419	8000.140967	14.145728	-0.053869	4.815543
258.540771	8000.111501	14.150733	-0.053826	4.815536
258.684297	8000.134171	14.155738	-0.053853	4.815542
258.818721	8000.159896	14.160743	-0.053878	4.815548
258.515680	8000.112217	14.165747	-0.053822	4.815536
258.533412	8000.116800	14.170752	-0.053825	4.815537
258.627650	8000.134389	14.175757	-0.053843	4.815542
258.688042	8000.188811	14.180762	-0.053855	4.815557
258.507195	8000.169841	14.185767	-0.053821	4.815553
258.541116	8000.159734	14.190771	-0.053828	4.815550
258.652723	8000.140219	14.195776	-0.053849	4.815543
258.382960	8000.105904	14.200781	-0.053799	4.815535
258.590155	8000.163802	14.205786	-0.053838	4.815551
258.559385	8000.163317	14.210791	-0.053832	4.815551
258.607386	8000.157714	14.215795	-0.053841	4.815549
258.425974	8000.180396	14.220800	-0.053808	4.815556
258.340655	8000.121332	14.225805	-0.053792	4.815539
258.531383	7999.202616	14.230810	-0.053827	4.815270

258.439779	7995.976631	14.235815	-0.053808	4.814327
258.439977	7990.534134	14.240819	-0.053805	4.812736
258.520147	7983.927184	14.245824	-0.053816	4.810803
258.370791	7976.594924	14.250829	-0.053783	4.808658
258.350417	7968.975871	14.255834	-0.053775	4.806428
258.363048	7961.201023	14.260839	-0.053772	4.804151
258.309650	7953.376663	14.265843	-0.053758	4.801858
258.375098	7945.361958	14.270848	-0.053765	4.799509
258.048909	7937.459199	14.275853	-0.053699	4.797192
258.224749	7929.379499	14.280858	-0.053727	4.794820
258.294846	7921.436157	14.285863	-0.053735	4.792488
258.293204	7913.345814	14.290867	-0.053730	4.790111
258.313470	7905.432919	14.295872	-0.053728	4.787786
257.967443	7897.359543	14.300877	-0.053659	4.785413
257.758209	7889.380250	14.305882	-0.053615	4.783067
257.840332	7881.391933	14.310887	-0.053625	4.780715
257.961340	7873.409102	14.315891	-0.053643	4.778364
257.817745	7865.456350	14.320896	-0.053611	4.776022
257.949698	7857.348057	14.325901	-0.053631	4.773631
257.833266	7849.373973	14.330906	-0.053604	4.771280
257.714232	7841.342484	14.335911	-0.053577	4.768911
257.631852	7833.392677	14.340915	-0.053556	4.766564
257.809006	7825.371779	14.345920	-0.053584	4.764195
257.850558	7817.395440	14.350925	-0.053587	4.761837
257.627775	7809.372420	14.355930	-0.053541	4.759466
257.513869	7801.432839	14.360935	-0.053515	4.757118
257.653353	7793.395702	14.365939	-0.053536	4.754739
257.603156	7785.292952	14.370944	-0.053521	4.752340
257.364941	7777.255470	14.375949	-0.053472	4.749960
257.473577	7769.334334	14.380954	-0.053487	4.747612
257.356951	7761.341011	14.385959	-0.053460	4.745242
257.398840	7753.328138	14.390963	-0.053463	4.742865
257.393331	7745.361902	14.395968	-0.053457	4.740500
257.258991	7737.384695	14.400973	-0.053427	4.738131
257.325141	7729.311615	14.405978	-0.053434	4.735733
257.373814	7721.351633	14.410983	-0.053439	4.733366
257.171869	7713.288311	14.415987	-0.053396	4.730968
257.185901	7705.352832	14.420992	-0.053394	4.728607
257.021164	7697.287608	14.425997	-0.053358	4.726206
256.997302	7689.258189	14.431002	-0.053348	4.723814
257.078764	7681.323834	14.436007	-0.053359	4.721449
257.048835	7673.276298	14.441011	-0.053348	4.719050
257.021007	7665.399239	14.446016	-0.053338	4.716700
256.988771	7657.329500	14.451021	-0.053327	4.714291
257.031222	7649.283308	14.456026	-0.053330	4.711888
257.016723	7641.265845	14.461031	-0.053322	4.709493
256.873335	7633.283872	14.466035	-0.053290	4.707107
256.898635	7625.280113	14.471040	-0.053290	4.704713
256.768696	7617.317910	14.476045	-0.053261	4.702331
256.889686	7609.272930	14.481050	-0.053278	4.699922
256.835796	7601.356933	14.486055	-0.053263	4.697550
256.747767	7593.284359	14.491059	-0.053242	4.695131
256.682007	7585.294196	14.496064	-0.053225	4.692735
256.658783	7577.284480	14.501069	-0.053216	4.690332
256.438566	7569.269393	14.506074	-0.053170	4.687927
256.335129	7561.272697	14.511079	-0.053145	4.685525
256.431008	7553.261524	14.516083	-0.053158	4.683118
256.608717	7545.321328	14.521088	-0.053186	4.680731
256.477831	7537.307770	14.526093	-0.053157	4.678320
256.376983	7529.297514	14.531098	-0.053133	4.675910
256.321618	7521.249153	14.536103	-0.053118	4.673487
256.164614	7513.152726	14.541107	-0.053083	4.671048
256.205255	7505.167090	14.546112	-0.053086	4.668641
256.099936	7497.206684	14.551117	-0.053061	4.666240
256.236942	7489.189332	14.556122	-0.053082	4.663821
256.139600	7481.277553	14.561127	-0.053059	4.661433
256.022938	7473.197231	14.566131	-0.053032	4.658992
255.967835	7465.290792	14.571136	-0.053017	4.656603
256.097504	7457.236262	14.576141	-0.053036	4.654167
256.010076	7449.231671	14.581146	-0.053015	4.651746
256.120258	7441.213294	14.586151	-0.053030	4.649319
255.784136	7433.221582	14.591155	-0.052963	4.646899
255.812930	7425.222713	14.596160	-0.052963	4.644475
255.745949	7417.266923	14.601165	-0.052946	4.642064
255.421758	7409.197451	14.606170	-0.052880	4.639616
255.477180	7401.255483	14.611175	-0.052886	4.637206
255.468739	7393.191082	14.616179	-0.052879	4.634758
255.581669	7385.188672	14.621184	-0.052895	4.632326
255.373037	7377.134554	14.626189	-0.052851	4.629879
255.345704	7369.160936	14.631194	-0.052841	4.627454
255.370318	7361.158739	14.636199	-0.052841	4.625019
255.518350	7353.194678	14.641203	-0.052863	4.622594
255.591838	7345.218311	14.646208	-0.052872	4.620165
255.502158	7337.213289	14.651213	-0.052850	4.617725
255.299560	7329.164412	14.656218	-0.052808	4.615271
255.583717	7321.155691	14.661223	-0.052856	4.612828
255.461388	7313.122575	14.666227	-0.052828	4.610376
255.508568	7305.177520	14.671232	-0.052832	4.607949
255.252692	7297.163282	14.676237	-0.052779	4.605500
255.284999	7289.201162	14.681242	-0.052780	4.603066
255.186845	7281.199505	14.686247	-0.052757	4.600619
254.999053	7273.186963	14.691251	-0.052717	4.598166
255.004438	7265.184622	14.696256	-0.052713	4.595716
255.104794	7257.114076	14.701261	-0.052726	4.593243
254.997060	7249.110324	14.706266	-0.052701	4.590789
255.193551	7241.118440	14.711271	-0.052733	4.588338
255.032745	7233.082714	14.716275	-0.052698	4.585872
255.024316	7225.127261	14.721280	-0.052691	4.583430
254.854097	7217.138882	14.726285	-0.052655	4.580975
255.043034	7209.134576	14.731290	-0.052685	4.578515
255.110266	7201.164298	14.736295	-0.052693	4.576064
254.845045	7193.102952	14.741299	-0.052638	4.573584
254.721449	7185.124695	14.746304	-0.052610	4.571127
254.684114	7177.089684	14.751309	-0.052598	4.568652
254.665307	7169.105564	14.756314	-0.052590	4.566191
254.520149	7161.105003	14.761319	-0.052558	4.563724
254.849679	7153.164545	14.766323	-0.052614	4.561274
254.904509	7145.122242	14.771328	-0.052619	4.558792
254.661715	7137.202861	14.776333	-0.052569	4.556345
254.466653	7129.118951	14.781338	-0.052528	4.553847
254.473109	7121.095103	14.786343	-0.052524	4.551366
254.359162	7113.062124	14.791347	-0.052498	4.548880
254.233606	7105.142544	14.796352	-0.052469	4.546429
254.343693	7097.099030	14.801357	-0.052485	4.543938
254.518361	7089.137079	14.806362	-0.052512	4.541471
254.350381	7081.145160	14.811367	-0.052476	4.538992
254.085691	7073.134118	14.816371	-0.052422	4.536507
254.355236	7065.116201	14.821376	-0.052467	4.534018
254.385047	7057.081016	14.826381	-0.052468	4.531523
254.357859	7049.125963	14.831386	-0.052458	4.529051
254.325099	7041.131138	14.836391	-0.052446	4.526565
253.930618	7033.069017	14.841395	-0.052368	4.524056
254.010819	7025.195626	14.846400	-0.052378	4.521606
253.929215	7017.084139	14.851405	-0.052358	4.519080
253.921604	7009.156963	14.856410	-0.052351	4.516609
253.711190	7001.065527	14.861415	-0.052307	4.514086
253.656018	6992.999479	14.866419	-0.052292	4.511570
253.869872	6985.046757	14.871424	-0.052327	4.509088
253.641971	6977.034075	14.876429	-0.052279	4.506585
253.604904	6969.057269	14.881434	-0.052267	4.504093
253.670850	6961.124930	14.886439	-0.052275	4.501613
253.510365	6953.027357	14.891443	-0.052240	4.499079
253.394624	6945.065636	14.896448	-0.052213	4.496587
253.362171	6937.042823	14.901453	-0.052202	4.494075
253.426878	6929.060446	14.906458	-0.052209	4.491573
253.561190	6921.063901	14.911463	-0.052229	4.489067
253.471421	6913.047137	14.916467	-0.052208	4.486552
253.526291	6905.068252	14.921472	-0.052213	4.484048
253.445529	6897.105147	14.926477	-0.052193	4.481547
253.220764	6889.064603	14.931482	-0.052146	4.479019
253.251288	6881.095453	14.936487	-0.052147	4.476514
252.989908	6873.006943	14.941491	-0.052093	4.473969
253.090406	6865.023254	14.946496	-0.052107	4.471456
252.995287	6857.030369	14.951501	-0.052084	4.468938
252.972728	6848.987716	14.956506	-0.052075	4.466404
252.885534	6841.028601	14.961511	-0.052054	4.463894
252.857878	6833.057469	14.966515	-0.052043	4.461379
253.045803	6825.065511	14.971520	-0.052073	4.458857
253.101211	6817.045042	14.976525	-0.052079	4.456325
252.911590	6809.008462	14.981530	-0.052038	4.453784
252.866014	6801.030009	14.986535	-0.052025	4.451261
252.898667	6793.021559	14.991539	-0.052026	4.448728
252.868182	6785.035249	14.996544	-0.052015	4.446200
252.694720	6776.985426	15.001549	-0.051978	4.443649
252.720473	6769.024297	15.006554	-0.051978	4.441126
252.610017	6761.064620	15.011559	-0.051952	4.438602
252.512258	6753.032617	15.016563	-0.051929	4.436053
252.547953	6744.963102	15.021568	-0.051931	4.433491
252.276198	6736.949768	15.026573	-0.051875	4.430945
252.271731	6728.940260	15.031578	-0.051869	4.428399
252.279618	6720.934205	15.036583	-0.051866	4.425853
252.499781	6712.967882	15.041587	-0.051902	4.423319
252.367650	6705.040723	15.046592	-0.051872	4.420795
252.117011	6697.012174	15.051597	-0.051821	4.418236
252.210003	6688.994862	15.056602	-0.051833	4.415681
252.266135	6680.984690	15.061607	-0.051838	4.413127
252.168294	6672.946354	15.066611	-0.051815	4.410561
252.115860	6664.996082	15.071616	-0.051800	4.408022
252.188008	6657.013242	15.076621	-0.051809	4.405472
252.045927	6649.017017	15.081626	-0.051777	4.402915
252.055952	6641.028846	15.086631	-0.051774	4.400360
251.900364	6632.976894	15.091635	-0.051740	4.397782
251.973199	6625.022362	15.096640	-0.051749	4.395235
251.667924	6616.990240	15.101645	-0.051687	4.392660
251.766251	6608.930674	15.106650	-0.051700	4.390077
251.683539	6600.955843	15.111655	-0.051680	4.387518
251.629345	6592.939502	15.116659	-0.051665	4.384944
251.948912	6585.008679	15.121664	-0.051719	4.382399
251.864825	6576.992512	15.126669	-0.051699	4.379822
251.439343	6569.007715	15.131674	-0.051615	4.377252
251.377114	6561.019146	15.136679	-0.051598	4.374682
251.560845	6552.997760	15.141683	-0.051627	4.372100
251.424483	6544.991916	15.146688	-0.051597	4.369521
251.322089	6536.989248	15.151693	-0.051573	4.366941
251.511357	6528.957689	15.156698	-0.051603	4.364352
251.569043	6521.034935	15.161703	-0.051609	4.361795
251.251664	6512.957906	15.166707	-0.051545	4.359185
251.186538	6505.041215	15.171712	-0.051528	4.356627
251.256223	6496.953697	15.176717	-0.051535	4.354013
251.282600	6488.889257	15.181722	-0.051535	4.351405
251.179673	6480.919071	15.186727	-0.051511	4.348824
251.184958	6472.900360	15.191731	-0.051507	4.346227
251.152597	6464.978728	15.196736	-0.051496	4.343660
251.012621	6456.994750	15.201741	-0.051465	4.341070
251.065266	6448.977855	15.206746	-0.051470	4.338470
251.272968	6440.994172	15.211751	-0.051504	4.335880
251.070732	6432.961558	15.216755	-0.051461	4.333269
251.114139	6424.926615	15.221760	-0.051464	4.330658
251.025227	6416.956990	15.226765	-0.051443	4.328065
250.782593	6408.916937	15.231770	-0.051392	4.325447
250.627600	6400.971919	15.236775	-0.051359	4.322859
250.815250	6392.901401	15.241779	-0.051388	4.320231
251.057775	6385.005847	15.246784	-0.051429	4.317659
250.878798	6376.981997	15.251789	-0.051390	4.315040
250.731550	6368.965234	15.256794	-0.051358	4.312422
250.856587	6360.916486	15.261799	-0.051376	4.309794
250.434745	6352.887353	15.266803	-0.051293	4.307167
250.502354	6344.921385	15.271808	-0.051300	4.304563
250.544479	6336.968457	15.276813	-0.051303	4.301961
250.467009	6328.910721	15.281818	-0.051284	4.299322
250.611774	6321.011682	15.286823	-0.051306	4.296736
250.496090	6312.899014	15.291827	-0.051279	4.294075
250.530996	6304.927592	15.296832	-0.051281	4.291461
250.278651	6296.877814	15.301837	-0.051229	4.288817
250.113086	6288.906966	15.306842	-0.051193	4.286198
250.192751	6280.954825	15.311847	-0.051203	4.283585
250.126317	6272.932440	15.316851	-0.051185	4.280947
250.047961	6264.918186	15.321856	-0.051166	4.278309
250.272767	6256.942805	15.326861	-0.051203	4.275686
250.153765	6248.887376	15.331866	-0.051175	4.273031
249.997520	6240.903316	15.336871	-0.051141	4.270398
249.916173	6232.853199	15.341875	-0.051121	4.267742
250.062059	6224.888150	15.346880	-0.051143	4.265115
249.978294	6216.892521	15.351885	-0.051123	4.262473
249.953539	6208.878575	15.356890	-0.051113	4.259825
250.042062	6200.962833	15.361895	-0.051125	4.257208
249.804284	6192.905204	15.366899	-0.051075	4.254540
249.918813	6184.894880	15.371904	-0.051092	4.251890
249.778022	6176.904131	15.376909	-0.051061	4.249241
249.811579	6168.891903	15.381914	-0.051062	4.246586
249.685755	6160.966321	15.386919	-0.051033	4.243956
249.501836	6152.940154	15.391923	-0.050994	4.241290
249.667867	6144.953306	15.396928	-0.051020	4.238639
249.500802	6136.924605	15.401933	-0.050984	4.235970
249.336512	6128.911285	15.406938	-0.050948	4.233303
249.492806	6120.891885	15.411943	-0.050973	4.230636
249.591654	6112.908227	15.416947	-0.050986	4.227979
249.338810	6104.925870	15.421952	-0.050934	4.225318
249.300944	6096.960062	15.426957	-0.050922	4.222662
249.495822	6088.920295	15.431962	-0.050953	4.219982
249.334412	6080.989775	15.436967	-0.050918	4.217333
249.403678	6072.909691	15.441971	-0.050926	4.214635
249.479311	6064.934487	15.446976	-0.050935	4.211970
249.262297	6056.902346	15.451981	-0.050890	4.209282
249.060997	6048.954221	15.456986	-0.050847	4.206620
249.177286	6040.972470	15.461991	-0.050864	4.203949
249.102592	6032.967251	15.466995	-0.050845	4.201266
249.256938	6024.958127	15.472000	-0.050869	4.198582
249.234631	6016.970814	15.477005	-0.050860	4.195902
249.258417	6008.853282	15.482010	-0.050859	4.193177
249.141453	6000.829144	15.487015	-0.050832	4.190480
249.046583	5992.847582	15.492019	-0.050810	4.187796
248.981437	5984.898984	15.497024	-0.050792	4.185122
248.777680	5976.919215	15.502029	-0.050750	4.182434
248.864692	5968.873978	15.507034	-0.050761	4.179725
248.899692	5960.943067	15.512039	-0.050762	4.177053
248.750262	5952.890996	15.517043	-0.050729	4.174336
248.534252	5944.938943	15.522048	-0.050684	4.171650
248.660521	5936.890048	15.527053	-0.050703	4.168934
248.588174	5928.880765	15.532058	-0.050684	4.166226
248.559085	5920.922333	15.537063	-0.050674	4.163535
248.316106	5912.921016	15.542067	-0.050624	4.160825
248.386390	5904.931783	15.547072	-0.050632	4.158121
248.312433	5896.933357	15.552077	-0.050613	4.155411
248.252106	5888.902888	15.557082	-0.050597	4.152688
248.293785	5880.875079	15.562087	-0.050600	4.149965
248.279059	5872.877493	15.567091	-0.050592	4.147250
248.238090	5864.885165	15.572096	-0.050579	4.144535
247.986879	5856.930349	15.577101	-0.050527	4.141828
248.072610	5848.884402	15.582106	-0.050538	4.139093
248.035716	5840.962772	15.587111	-0.050527	4.136396
248.043068	5832.855036	15.592115	-0.050523	4.133635
248.036934	5824.857611	15.597120	-0.050517	4.130910
248.006469	5816.888325	15.602125	-0.050506	4.128192
247.800966	5808.875846	15.607130	-0.050463	4.125455
247.758080	5800.922193	15.612135	-0.050450	4.122739
247.653460	5792.889323	15.617139	-0.050425	4.119992
247.753146	5784.935490	15.622144	-0.050439	4.117274
247.848583	5776.960582	15.627149	-0.050452	4.114547
247.703205	5768.858696	15.632154	-0.050420	4.111771
247.678636	5760.858894	15.637159	-0.050410	4.109030
247.331686	5752.862133	15.642163	-0.050340	4.106284
247.763987	5744.855666	15.647168	-0.050416	4.103543
247.540500	5736.914095	15.652173	-0.050369	4.100813
247.508572	5728.906018	15.657178	-0.050358	4.098062
247.388619	5720.934895	15.662183	-0.050331	4.095320
247.549679	5712.893802	15.667187	-0.050356	4.092556
247.491699	5704.903831	15.672192	-0.050340	4.089805
247.448481	5696.917780	15.677197	-0.050327	4.087054
247.254156	5688.877916	15.682202	-0.050286	4.084280
247.361459	5680.970957	15.687207	-0.050301	4.081554
246.992756	5672.931822	15.692211	-0.050228	4.078774
247.125493	5664.981216	15.697216	-0.050247	4.076030
247.354751	5656.939018	15.702221	-0.050285	4.073254
246.874386	5648.908404	15.707226	-0.050190	4.070469
247.233903	5640.925952	15.712231	-0.050252	4.067712
247.088365	5632.891929	15.717235	-0.050220	4.064927
247.132405	5624.968253	15.722240	-0.050224	4.062182
246.968523	5616.943318	15.727245	-0.050188	4.059396
246.964730	5608.965888	15.732250	-0.050182	4.056628
247.062692	5600.958218	15.737255	-0.050196	4.053848
246.754917	5592.928989	15.742259	-0.050133	4.051053
246.684942	5584.952869	15.747264	-0.050115	4.048278
246.746609	5576.963239	15.752269	-0.050122	4.045499
246.706887	5568.966358	15.757274	-0.050109	4.042713
246.754390	5560.973979	15.762279	-0.050113	4.039929
246.746827	5552.973346	15.767283	-0.050107	4.037139
246.588171	5544.959715	15.772288	-0.050072	4.034340
246.275747	5536.843971	15.777293	-0.050009	4.031501
246.234781	5528.873224	15.782298	-0.049996	4.028715
246.444085	5520.903347	15.787303	-0.050030	4.025931
246.350355	5512.887965	15.792307	-0.050008	4.023125
246.147899	5504.925782	15.797312	-0.049965	4.020333
246.349864	5496.956693	15.802317	-0.049998	4.017544
246.172419	5488.899545	15.807322	-0.049960	4.014716
246.264348	5480.909074	15.812327	-0.049972	4.011913
245.935774	5472.894101	15.817331	-0.049906	4.009093
245.957466	5464.910902	15.822336	-0.049905	4.006288
246.174123	5456.920938	15.827341	-0.049940	4.003482
245.992714	5448.933261	15.832346	-0.049902	4.000668
245.997092	5440.964094	15.837351	-0.049897	3.997862
245.700148	5432.931950	15.842355	-0.049837	3.995026
245.695982	5424.933784	15.847360	-0.049831	3.992205
245.708961	5416.887430	15.852365	-0.049829	3.989366
245.539574	5408.923297	15.857370	-0.049792	3.986551
245.623128	5400.900120	15.862375	-0.049803	3.983716
245.411062	5392.944081	15.867379	-0.049758	3.980899
245.382935	5384.987790	15.872384	-0.049748	3.978083
245.623433	5376.975155	15.877389	-0.049788	3.975249
245.576957	5368.939443	15.882394	-0.049774	3.972400
245.644201	5360.905882	15.887399	-0.049782	3.969552
245.467912	5352.945070	15.892403	-0.049744	3.966723
245.439092	5344.939904	15.897408	-0.049734	3.963879
245.456696	5336.971635	15.902413	-0.049732	3.961047
245.333235	5328.985162	15.907418	-0.049704	3.958205
245.274359	5321.018892	15.912423	-0.049688	3.955368
245.154533	5312.951817	15.917427	-0.049661	3.952492
245.113641	5304.937594	15.922432	-0.049648	3.949635
245.128488	5296.993825	15.927437	-0.049646	3.946801
244.762160	5288.987101	15.932442	-0.049573	3.943936
245.026846	5280.987497	15.937447	-0.049617	3.941083
244.873169	5272.996003	15.942451	-0.049583	3.938223
244.888294	5264.995001	15.947456	-0.049581	3.935361
244.715489	5257.011830	15.952461	-0.049544	3.932500
244.783839	5248.946666	15.957466	-0.049552	3.929611
244.614675	5241.001212	15.962471	-0.049515	3.926759
244.661381	5232.981980	15.967475	-0.049519	3.923883
244.697753	5225.018679	15.972480	-0.049521	3.921024
244.618519	5217.053173	15.977485	-0.049501	3.918160
244.588341	5209.024197	15.982490	-0.049490	3.915272
244.817388	5200.997393	15.987495	-0.049528	3.912388
244.586829	5192.942914	15.992499	-0.049480	3.909483
244.459462	5185.001756	15.997504	-0.049451	3.906618
244.535933	5176.989271	16.002509	-0.049461	3.903730
244.695574	5168.979221	16.007514	-0.049485	3.900842
244.368180	5161.023848	16.012519	-0.049419	3.897962
244.240142	5152.997554	16.017523	-0.049391	3.895058
244.249000	5145.013227	16.022528	-0.049387	3.892170
244.245662	5136.988061	16.027533	-0.049382	3.889265
244.133151	5128.986755	16.032538	-0.049356	3.886364
244.080558	5120.999475	16.037543	-0.049341	3.883467
244.125493	5113.014688	16.042547	-0.049344	3.880571
243.936632	5105.038084	16.047552	-0.049304	3.877671
243.896368	5097.038918	16.052557	-0.049292	3.874763
243.903984	5088.766002	16.057562	-0.049288	3.871755
243.916157	5080.852565	16.062567	-0.049285	3.868875
243.905419	5072.868292	16.067571	-0.049278	3.865967
243.884809	5064.935101	16.072576	-0.049269	3.863075
243.895219	5056.978786	16.077581	-0.049266	3.860173
243.860881	5048.993301	16.082586	-0.049255	3.857257
243.740810	5041.010920	16.087591	-0.049228	3.854339
243.744910	5033.008981	16.092595	-0.049223	3.851414
243.522907	5025.002669	16.097600	-0.049177	3.848480
243.542063	5017.010415	16.102605	-0.049176	3.845554
243.613705	5009.007676	16.107610	-0.049184	3.842623
243.542968	5001.047103	16.112615	-0.049166	3.839702
243.376117	4993.084435	16.117619	-0.049130	3.836777
243.515504	4985.045164	16.122624	-0.049151	3.833827
243.656619	4977.028911	16.127629	-0.049172	3.830884
243.343482	4969.042092	16.132634	-0.049109	3.827939
243.217359	4961.052566	16.137639	-0.049080	3.824996
243.389173	4953.082662	16.142643	-0.049107	3.822063
243.386852	4945.066188	16.147648	-0.049102	3.819108
243.309023	4937.118647	16.152653	-0.049083	3.816173
243.407627	4929.062239	16.157658	-0.049096	3.813201
243.149536	4921.096990	16.162663	-0.049043	3.810252
242.881398	4913.105700	16.167667	-0.048988	3.807290
242.971274	4905.072823	16.172672	-0.049000	3.804319
242.875081	4897.147259	16.177677	-0.048977	3.801381
242.855044	4889.087846	16.182682	-0.048968	3.798393
242.918870	4881.140030	16.187687	-0.048975	3.795446
242.878451	4873.080146	16.192691	-0.048962	3.792453
242.912274	4865.051629	16.197696	-0.048964	3.789470
242.651555	4857.081406	16.202701	-0.048910	3.786501
242.818934	4849.083543	16.207706	-0.048936	3.783528
242.962557	4841.084109	16.212711	-0.048958	3.780552
242.580699	4833.120903	16.217715	-0.048882	3.777575
242.544686	4825.104760	16.222720	-0.048870	3.774584
242.778722	4817.104532	16.227725	-0.048909	3.771602
242.277846	4809.110970	16.232730	-0.048811	3.768604
242.401275	4801.110099	16.237735	-0.048829	3.765615
242.337408	4793.132835	16.242739	-0.048812	3.762628
242.465385	4785.082667	16.247744	-0.048831	3.759616
242.289364	4777.165029	16.252749	-0.048793	3.756644
242.357799	4769.105527	16.257754	-0.048801	3.753623
242.478948	4761.104916	16.262759	-0.048818	3.750622
242.317689	4753.116593	16.267763	-0.048783	3.747616
242.259784	4745.090133	16.272768	-0.048767	3.744597
242.260392	4737.180122	16.277773	-0.048763	3.741620
242.079075	4729.143658	16.282778	-0.048724	3.738589
242.065330	4721.157889	16.287783	-0.048716	3.735578
242.290307	4713.126269	16.292787	-0.048753	3.732554
241.994847	4705.126593	16.297792	-0.048693	3.729526
241.829608	4697.174827	16.302797	-0.048657	3.726518
241.834046	4689.158508	16.307802	-0.048653	3.723486
242.054625	4681.208288	16.312807	-0.048689	3.720482
241.898226	4673.223481	16.317811	-0.048655	3.717454
241.902789	4665.186337	16.322816	-0.048651	3.714407
242.010348	4657.108844	16.327821	-0.048666	3.711345
241.881859	4649.106666	16.332826	-0.048637	3.708304
241.541640	4641.147848	16.337831	-0.048569	3.705271
241.484622	4633.167424	16.342835	-0.048553	3.702234
241.550412	4625.182283	16.347840	-0.048560	3.699196
241.351771	4617.245565	16.352845	-0.048518	3.696167
241.480299	4609.180197	16.357850	-0.048537	3.693095
241.503404	4601.197125	16.362855	-0.048537	3.690049
241.461688	4593.201225	16.367859	-0.048524	3.686994
241.432154	4585.205454	16.372864	-0.048513	3.683937
241.360244	4577.265651	16.377869	-0.048495	3.680898
241.187232	4569.251968	16.382874	-0.048458	3.677825
241.235676	4561.282386	16.387879	-0.048462	3.674773
241.304076	4553.225311	16.392883	-0.048470	3.671684
241.192080	4545.241587	16.397888	-0.048444	3.668617
241.314475	4537.236611	16.402893	-0.048462	3.665545
241.219981	4529.237538	16.407898	-0.048439	3.662467
241.428142	4521.227152	16.412903	-0.048473	3.659390
241.116186	4513.277412	16.417907	-0.048410	3.656320
241.196792	4505.251058	16.422912	-0.048420	3.653228
241.213302	4497.258499	16.427917	-0.048418	3.650145
240.955738	4489.255113	16.432922	-0.048365	3.647048
241.000937	4481.277398	16.437927	-0.048368	3.643967
240.976358	4473.310420	16.442931	-0.048359	3.640885
240.845683	4465.318845	16.447936	-0.048329	3.637788
240.848809	4457.325668	16.452941	-0.048325	3.634691
240.886964	4449.241907	16.457946	-0.048327	3.631557
240.809634	4441.286539	16.462951	-0.048308	3.628468
240.564071	4433.282264	16.467955	-0.048257	3.625352
240.528448	4425.312007	16.472960	-0.048245	3.622252
240.645834	4417.316181	16.477965	-0.048262	3.619144
240.752567	4409.317511	16.482970	-0.048277	3.616032
240.534042	4401.343072	16.487975	-0.048232	3.612918
240.353987	4393.305690	16.492979	-0.048193	3.609778
240.409163	4385.329002	16.497984	-0.048198	3.606665
240.311304	4377.340542	16.502989	-0.048175	3.603540
240.343205	4369.352179	16.507994	-0.048176	3.600417
240.297251	4361.421758	16.512999	-0.048163	3.597311
240.316848	4353.370844	16.518003	-0.048161	3.594157
239.989062	4345.370323	16.523008	-0.048095	3.591011
240.097091	4337.375698	16.528013	-0.048110	3.587876
240.233114	4329.362158	16.533018	-0.048131	3.584732
240.012048	4321.447400	16.538023	-0.048084	3.581613
239.914358	4313.418053	16.543027	-0.048061	3.578451
239.958937	4305.422703	16.548032	-0.048065	3.575303
240.051213	4297.422973	16.553037	-0.048077	3.572152
239.760607	4289.406169	16.558042	-0.048018	3.568980
239.983197	4281.442620	16.563047	-0.048054	3.565842
239.769290	4273.451088	16.568051	-0.048009	3.562676
239.722234	4265.416555	16.573056	-0.047996	3.559496
239.879127	4257.465518	16.578061	-0.048020	3.556353
239.661593	4249.380006	16.583066	-0.047974	3.553142
239.696475	4241.348379	16.588071	-0.047976	3.549957
239.384981	4233.408788	16.593075	-0.047913	3.546795
239.429653	4225.401829	16.598080	-0.047916	3.543614
239.294934	4217.442982	16.603085	-0.047886	3.540444
239.306424	4209.455232	16.608090	-0.047883	3.537265
239.429890	4201.436449	16.613095	-0.047901	3.534073
239.276371	4193.452091	16.618099	-0.047868	3.530884
239.469102	4185.456554	16.623104	-0.047899	3.527698
239.263515	4177.453173	16.628109	-0.047855	3.524494
239.223799	4169.492110	16.633114	-0.047843	3.521309
239.255006	4161.514918	16.638119	-0.047844	3.518116
239.131247	4153.508552	16.643123	-0.047816	3.514905
239.183967	4145.492884	16.648128	-0.047821	3.511692
239.006896	4137.508463	16.653133	-0.047783	3.508482
238.843743	4129.507058	16.658138	-0.047747	3.505262
238.921766	4121.544844	16.663143	-0.047757	3.502062
238.823419	4113.546199	16.668147	-0.047733	3.498840
238.871701	4105.548206	16.673152	-0.047737	3.495619
238.857813	4097.573252	16.678157	-0.047730	3.492403
238.734406	4089.533817	16.683162	-0.047702	3.489154
238.901030	4081.579600	16.688167	-0.047728	3.485946
238.726784	4073.603869	16.693171	-0.047691	3.482715
238.593685	4065.593832	16.698176	-0.047661	3.479469
238.543308	4057.647191	16.703181	-0.047646	3.476248
238.450973	4049.615074	16.708186	-0.047624	3.472988
238.444940	4041.573698	16.713191	-0.047618	3.469724
238.481252	4033.612569	16.718195	-0.047620	3.466491
238.361585	4025.612211	16.723200	-0.047593	3.463234
238.402577	4017.638790	16.728205	-0.047595	3.459990
238.314537	4009.651773	16.733210	-0.047574	3.456733
238.552191	4001.620905	16.738215	-0.047613	3.453466
238.028444	3993.657334	16.743219	-0.047511	3.450198
237.995472	3985.640542	16.748224	-0.047499	3.446921
237.998171	3977.679628	16.753229	-0.047495	3.443666
237.960186	3969.657891	16.758234	-0.047483	3.440381
238.049151	3961.705862	16.763239	-0.047495	3.437125
237.996494	3953.692225	16.768243	-0.047480	3.433837
237.873757	3945.663134	16.773248	-0.047452	3.430537
237.917592	3937.685902	16.778253	-0.047455	3.427260
238.088909	3929.655746	16.783258	-0.047482	3.423963
237.894422	3921.752028	16.788263	-0.047441	3.420702
237.697601	3913.774356	16.793267	-0.047399	3.417408
237.703105	3905.730253	16.798272	-0.047395	3.414090
237.760283	3897.720675	16.803277	-0.047401	3.410785
237.612957	3889.733561	16.808282	-0.047368	3.407479
237.602220	3881.741390	16.813287	-0.047361	3.404172
237.629514	3873.789237	16.818291	-0.047362	3.400880
237.587075	3865.805441	16.823296	-0.047349	3.397569
237.715945	3857.821858	16.828301	-0.047368	3.394261
237.650847	3849.694757	16.833306	-0.047351	3.390883
237.488123	3841.735625	16.838311	-0.047315	3.387568
237.266246	3833.775860	16.843315	-0.047269	3.384248
237.117668	3825.824555	16.848320	-0.047236	3.380931
237.266108	3817.840973	16.853325	-0.047259	3.377607
237.168516	3809.821052	16.858330	-0.047236	3.374256
237.063519	3801.820982	16.863335	-0.047211	3.370910
237.164593	3793.844891	16.868339	-0.047225	3.367578
236.970109	3785.835603	16.873344	-0.047184	3.364218
237.093595	3777.900965	16.878349	-0.047202	3.360897
236.840840	3769.900822	16.883354	-0.047150	3.357532
237.137586	3761.888235	16.888359	-0.047200	3.354179
236.783074	3753.881109	16.893363	-0.047129	3.350801
236.873895	3745.870390	16.898368	-0.047141	3.347433
236.941432	3737.865266	16.903373	-0.047149	3.344064
236.975736	3729.908818	16.908378	-0.047150	3.340711
236.693062	3721.968736	16.913383	-0.047092	3.337350
236.788329	3713.922539	16.918387	-0.047105	3.333955
236.917478	3705.904407	16.923392	-0.047124	3.330569
236.567831	3697.989437	16.928397	-0.047054	3.327206
236.546308	3689.980159	16.933402	-0.047045	3.323811
236.681352	3681.991769	16.938407	-0.047065	3.320428
236.321797	3674.048509	16.943411	-0.046993	3.317042
236.363471	3666.022242	16.948416	-0.046996	3.313632
236.420796	3657.993299	16.953421	-0.047002	3.310218
236.197278	3649.993174	16.958426	-0.046955	3.306802
236.352473	3642.018200	16.963431	-0.046979	3.303408
236.247082	3634.040977	16.968435	-0.046955	3.299999
236.204594	3626.063503	16.973440	-0.046942	3.296589
236.013114	3618.079206	16.978445	-0.046901	3.293167
235.970267	3610.039663	16.983450	-0.046888	3.289724
236.079304	3602.093907	16.988455	-0.046903	3.286323
235.887029	3594.096959	16.993459	-0.046863	3.282884
235.932270	3586.084833	16.998464	-0.046866	3.279445
235.883445	3578.173807	17.003469	-0.046852	3.276042
235.726062	3570.125727	17.008474	-0.046818	3.272572
235.783616	3562.098573	17.013479	-0.046823	3.269116
235.558972	3554.120807	17.018483	-0.046777	3.265667
235.775767	3546.143770	17.023488	-0.046812	3.262231
235.781896	3538.168333	17.028493	-0.046808	3.258785
235.696922	3530.173633	17.033498	-0.046787	3.255322
235.573970	3522.183772	17.038503	-0.046759	3.251857
235.575525	3514.175184	17.043507	-0.046755	3.248385
235.471384	3506.177734	17.048512	-0.046730	3.244909
235.502783	3498.235249	17.053517	-0.046731	3.241460
235.568132	3490.219151	17.058522	-0.046738	3.237975
235.222903	3482.277031	17.063527	-0.046669	3.234503
235.325988	3474.168014	17.068531	-0.046683	3.230972
235.274544	3466.204499	17.073536	-0.046669	3.227495
235.530625	3458.215843	17.078541	-0.046711	3.224016
235.023936	3450.258636	17.083546	-0.046612	3.220515
235.024963	3442.296162	17.088551	-0.046607	3.217029
235.134016	3434.285884	17.093555	-0.046623	3.213523
235.179758	3426.280310	17.098560	-0.046626	3.210012
235.034318	3418.345577	17.103565	-0.046594	3.206521
234.813483	3410.327355	17.108570	-0.046548	3.202986
234.994158	3402.333173	17.113575	-0.046577	3.199474
234.809441	3394.385241	17.118579	-0.046537	3.195964
234.889759	3386.358658	17.123584	-0.046547	3.192426
234.832134	3378.379531	17.128589	-0.046532	3.188899
234.633032	3370.379745	17.133594	-0.046490	3.185353
234.792134	3362.426544	17.138599	-0.046514	3.181840
234.731218	3354.414459	17.143603	-0.046498	3.178286
234.478834	3346.443149	17.148608	-0.046446	3.174739
234.607055	3338.450510	17.153613	-0.046465	3.171195
234.422254	3330.428912	17.158618	-0.046425	3.167620
234.264842	3322.464280	17.163623	-0.046391	3.164068
234.326688	3314.505614	17.168627	-0.046398	3.160524
234.269573	3306.515653	17.173632	-0.046382	3.156957
234.305386	3298.517324	17.178637	-0.046384	3.153386
234.138016	3290.463431	17.183642	-0.046348	3.149777
234.387439	3282.483356	17.188647	-0.046389	3.146215
234.129770	3274.517304	17.193651	-0.046336	3.142634
234.055592	3266.536895	17.198656	-0.046317	3.139050
234.229308	3258.585025	17.203661	-0.046345	3.135485
234.271002	3250.553131	17.208666	-0.046347	3.131875
234.202099	3242.592678	17.213671	-0.046330	3.128288
234.045629	3234.605752	17.218675	-0.046295	3.124681
234.185501	3226.629877	17.223680	-0.046317	3.121088
234.022192	3218.673194	17.228685	-0.046281	3.117485
233.752708	3210.684618	17.233690	-0.046226	3.113860
233.988884	3202.641992	17.238695	-0.046265	3.110228
233.812883	3194.681462	17.243699	-0.046227	3.106611
233.492692	3186.704166	17.248704	-0.046163	3.102976
233.561369	3178.732413	17.253709	-0.046170	3.099356
233.497252	3170.751732	17.258714	-0.046154	3.095722
233.336396	3162.745671	17.263719	-0.046119	3.092068
233.231074	3154.763399	17.268723	-0.046094	3.088422
233.572905	3146.729030	17.273728	-0.046153	3.084770
233.633079	3138.776881	17.278733	-0.046159	3.081137
233.302721	3130.807559	17.283738	-0.046092	3.077474
233.139925	3122.816570	17.288743	-0.046057	3.073805
233.181270	3114.749818	17.293747	-0.046060	3.070106
233.198460	3106.787611	17.298752	-0.046058	3.066450
233.117551	3098.821852	17.303757	-0.046038	3.062783
233.325669	3090.816434	17.308762	-0.046072	3.059106
233.230979	3082.888142	17.313767	-0.046049	3.055447
233.200019	3074.872940	17.318771	-0.046038	3.051746
232.889858	3066.904325	17.323776	-0.045976	3.048049
233.014805	3058.918865	17.328781	-0.045994	3.044361
232.795386	3050.975241	17.333786	-0.045948	3.040670
232.893465	3042.986302	17.338791	-0.045961	3.036970
232.995407	3034.956929	17.343795	-0.045975	3.033246
232.625766	3026.953491	17.348800	-0.045902	3.029507
232.650219	3019.012257	17.353805	-0.045901	3.025812
232.444908	3011.035060	17.358810	-0.045858	3.022084
232.670408	3003.040844	17.363815	-0.045895	3.018364
232.798745	2995.045172	17.368819	-0.045914	3.014635
232.651495	2987.043550	17.373824	-0.045881	3.010884
232.888728	2979.058201	17.378829	-0.045921	3.007156
232.479792	2971.114069	17.383834	-0.045840	3.003410
232.412752	2963.152639	17.388839	-0.045822	2.999668
232.478519	2955.159274	17.393843	-0.045829	2.995913
232.326209	2947.143971	17.398848	-0.045796	2.992133
232.305749	2939.167923	17.403853	-0.045787	2.988372
232.241790	2931.156964	17.408858	-0.045770	2.984588
232.237468	2923.218519	17.413863	-0.045765	2.980837
232.178923	2915.247713	17.418867	-0.045749	2.977063
231.916069	2907.266062	17.423872	-0.045695	2.973268
232.252404	2899.207597	17.428877	-0.045752	2.969463
231.961709	2891.268549	17.433882	-0.045693	2.965677
231.866193	2883.314235	17.438887	-0.045670	2.961890
231.964829	2875.323705	17.443891	-0.045684	2.958090
231.862692	2867.337547	17.448896	-0.045660	2.954277
231.738768	2859.370641	17.453901	-0.045632	2.950467
231.746829	2851.352168	17.458906	-0.045628	2.946635
231.729765	2843.378786	17.463911	-0.045620	2.942817
231.633855	2835.395025	17.468915	-0.045597	2.938986
231.671287	2827.413075	17.473920	-0.045599	2.935158
231.866702	2819.421713	17.478925	-0.045631	2.931328
231.708132	2811.420964	17.483930	-0.045596	2.927470
231.594064	2803.460302	17.488935	-0.045570	2.923629
231.488997	2795.502709	17.493939	-0.045545	2.919784
231.290613	2787.567183	17.498944	-0.045504	2.915940
231.516798	2779.474948	17.503949	-0.045541	2.912038
231.282185	2771.463496	17.508954	-0.045492	2.908145
231.169265	2763.518948	17.513959	-0.045466	2.904286
231.025532	2755.583285	17.518963	-0.045434	2.900425
230.974660	2747.613345	17.523968	-0.045420	2.896546
231.114316	2739.594540	17.528973	-0.045441	2.892649
231.002230	2731.599071	17.533978	-0.045415	2.888744
230.782709	2723.654540	17.538983	-0.045369	2.884853
230.955085	2715.688653	17.543987	-0.045396	2.880968
230.872105	2707.693106	17.548992	-0.045376	2.877049
230.913504	2699.715589	17.553997	-0.045379	2.873140
230.735288	2691.699154	17.559002	-0.045340	2.869195
230.757484	2683.729102	17.564007	-0.045340	2.865278
230.800198	2675.765093	17.569011	-0.045343	2.861360
230.575220	2667.807938	17.574016	-0.045296	2.857425
230.645093	2659.809013	17.579021	-0.045304	2.853480
230.383906	2651.822544	17.584026	-0.045250	2.849518
230.412335	2643.860552	17.589031	-0.045250	2.845578
230.418639	2635.895087	17.594035	-0.045247	2.841630
230.268338	2627.927047	17.599040	-0.045214	2.837667
230.337394	2619.937109	17.604045	-0.045222	2.833699
230.200532	2611.924128	17.609050	-0.045191	2.829702
230.235065	2603.947412	17.614055	-0.045192	2.825728
230.213076	2595.988986	17.619059	-0.045183	2.821754
230.124204	2588.007629	17.624064	-0.045162	2.817759
230.246140	2580.036512	17.629069	-0.045180	2.813776
230.054939	2572.024854	17.634074	-0.045139	2.809748
229.972197	2564.066366	17.639079	-0.045119	2.805748
229.856520	2556.131135	17.644083	-0.045092	2.801752
229.820086	2548.145467	17.649088	-0.045080	2.797729
229.641694	2540.179063	17.654093	-0.045042	2.793702
229.651690	2532.146806	17.659098	-0.045039	2.789647
229.673329	2524.171141	17.664103	-0.045038	2.785615
229.749694	2516.203726	17.669107	-0.045047	2.781585
229.552667	2508.247051	17.674112	-0.045006	2.777538
229.563128	2500.284018	17.679117	-0.045003	2.773495
229.495401	2492.264443	17.684122	-0.044985	2.769412
229.435021	2484.323853	17.689127	-0.044969	2.765363
229.334469	2476.371500	17.694131	-0.044945	2.761301
229.424237	2468.369475	17.699136	-0.044957	2.757218
229.492451	2460.358005	17.704141	-0.044965	2.753123
229.179691	2452.346068	17.709146	-0.044901	2.748999
229.312283	2444.354564	17.714151	-0.044921	2.744906
229.211258	2436.417085	17.719155	-0.044897	2.740821
229.107419	2428.453038	17.724160	-0.044873	2.736715
229.277348	2420.467928	17.729165	-0.044900	2.732610
229.277469	2412.479842	17.734170	-0.044895	2.728486
228.902708	2404.547223	17.739175	-0.044820	2.724361
228.795152	2396.619686	17.744179	-0.044795	2.720250
228.809223	2388.620500	17.749184	-0.044793	2.716102
228.835538	2380.633860	17.754189	-0.044793	2.711955
228.698422	2372.641207	17.759194	-0.044762	2.707789
228.624236	2364.670747	17.764199	-0.044743	2.703632
228.641604	2356.702783	17.769203	-0.044742	2.699475
228.541021	2348.758883	17.774208	-0.044718	2.695317
228.508014	2340.767301	17.779213	-0.044707	2.691132
228.574439	2332.765453	17.784218	-0.044714	2.686942
228.523737	2324.821696	17.789223	-0.044700	2.682767
228.225266	2316.888891	17.794227	-0.044639	2.678577
228.325736	2308.875864	17.799232	-0.044653	2.674363
228.341846	2300.863183	17.804237	-0.044651	2.670137
228.237809	2292.880744	17.809242	-0.044627	2.665912
228.275384	2284.917925	17.814247	-0.044629	2.661701
228.081572	2276.993571	17.819251	-0.044588	2.657488
227.921210	2269.010818	17.824256	-0.044553	2.653240
228.108765	2260.997168	17.829261	-0.044583	2.648991
228.087711	2253.033559	17.834266	-0.044574	2.644748
228.033499	2245.089733	17.839271	-0.044559	2.640506
227.984426	2237.137341	17.844275	-0.044545	2.636254
227.943802	2229.136145	17.849280	-0.044532	2.631969
227.723194	2221.180392	17.854285	-0.044486	2.627690
227.750419	2213.173397	17.859290	-0.044486	2.623393
227.714663	2205.240950	17.864295	-0.044474	2.619124
228.037016	2197.247521	17.869299	-0.044529	2.614840
227.740775	2189.283975	17.874304	-0.044469	2.610523
227.434986	2181.375938	17.879309	-0.044408	2.606228
227.476454	2173.378798	17.884314	-0.044410	2.601901
227.590745	2165.399076	17.889319	-0.044427	2.597582
227.535031	2157.382873	17.894323	-0.044411	2.593224
227.182364	2149.267990	17.899328	-0.044340	2.588785
227.388853	2141.308909	17.904333	-0.044374	2.584461
227.149011	2133.421616	17.909338	-0.044324	2.580138
227.207788	2125.471635	17.914343	-0.044330	2.575795
227.204857	2117.502362	17.919347	-0.044325	2.571429
227.070451	2109.529090	17.924352	-0.044295	2.567045
227.060151	2101.584203	17.929357	-0.044288	2.562677
227.039958	2093.651563	17.934362	-0.044279	2.558308
227.035645	2085.680417	17.939367	-0.044273	2.553911
226.975588	2077.685183	17.944371	-0.044257	2.549490
226.901725	2069.719412	17.949376	-0.044239	2.545076
227.010968	2061.774861	17.954381	-0.044254	2.540679
226.982520	2053.812956	17.959386	-0.044244	2.536255
226.753193	2045.863122	17.964391	-0.044196	2.531816
227.001016	2037.861052	17.969395	-0.044237	2.527374
226.780243	2029.907465	17.974400	-0.044191	2.522918
226.714275	2021.991711	17.979405	-0.044174	2.518486
226.591513	2014.022339	17.984410	-0.044146	2.514012
226.448426	2006.014266	17.989415	-0.044114	2.509506
226.526818	1998.029018	17.994419	-0.044124	2.505022
226.384307	1990.080694	17.999424	-0.044093	2.500534
226.333331	1982.148160	18.004429	-0.044078	2.496054
226.098295	1974.182808	18.009434	-0.044029	2.491534
225.970912	1966.208741	18.014439	-0.044001	2.487008
225.963403	1958.260091	18.019443	-0.043994	2.482497
226.170920	1950.261728	18.024448	-0.044028	2.477966
225.915289	1942.334848	18.029453	-0.043975	2.473433
225.742587	1934.352253	18.034458	-0.043938	2.468866
226.032874	1926.343741	18.039463	-0.043987	2.464310
225.776604	1918.441993	18.044467	-0.043935	2.459766
225.722934	1910.455626	18.049472	-0.043920	2.455180
225.875895	1902.482891	18.054477	-0.043943	2.450609
225.677289	1894.528569	18.059482	-0.043901	2.446013
225.633076	1886.587393	18.064487	-0.043888	2.441428
225.718634	1878.635432	18.069491	-0.043899	2.436838
225.639278	1870.622658	18.074496	-0.043879	2.432192
225.496663	1862.651599	18.079501	-0.043848	2.427556
225.464746	1854.685501	18.084506	-0.043837	2.422922
225.401155	1846.749022	18.089511	-0.043820	2.418295
225.216169	1838.810465	18.094515	-0.043781	2.413648
225.105022	1830.831090	18.099520	-0.043755	2.408973
225.239910	1822.872334	18.104525	-0.043775	2.404321
225.258768	1814.912728	18.109530	-0.043774	2.399650
225.234102	1806.970692	18.114535	-0.043764	2.394978
225.186927	1798.984980	18.119539	-0.043750	2.390268
225.060607	1791.021655	18.124544	-0.043722	2.385556
225.305895	1783.055184	18.129549	-0.043763	2.380863
224.935220	1775.160070	18.134554	-0.043689	2.376153
224.839909	1767.199732	18.139559	-0.043666	2.371417
224.901984	1759.228141	18.144563	-0.043673	2.366678
224.605621	1751.299327	18.149568	-0.043612	2.361926
224.840873	1743.333440	18.154573	-0.043651	2.357185
224.665413	1735.360529	18.159578	-0.043614	2.352397
224.683620	1727.377224	18.164583	-0.043612	2.347608
224.625215	1719.434055	18.169587	-0.043596	2.342828
224.516583	1711.491940	18.174592	-0.043571	2.338034
224.282211	1703.576288	18.179597	-0.043522	2.333237
224.454330	1695.556777	18.184602	-0.043549	2.328400
224.410782	1687.612524	18.189607	-0.043536	2.323580
224.241116	1679.705834	18.194611	-0.043500	2.318763
224.064886	1671.750480	18.199616	-0.043462	2.313906
224.351769	1663.733978	18.204621	-0.043510	2.309040
224.170554	1655.796033	18.209626	-0.043472	2.304173
224.155024	1647.855793	18.214631	-0.043464	2.299307
223.979600	1639.947222	18.219635	-0.043426	2.294438
224.082070	1631.939230	18.224640	-0.043440	2.289520
223.883560	1624.032082	18.229645	-0.043399	2.284628
223.659480	1616.102869	18.234650	-0.043352	2.279710
224.112972	1608.104809	18.239655	-0.043431	2.274797
224.014546	1600.076213	18.244659	-0.043408	2.269806
223.635083	1592.146904	18.249664	-0.043332	2.264842
223.664140	1584.222806	18.254669	-0.043333	2.259906
223.513438	1576.309268	18.259674	-0.043300	2.254950
223.499508	1568.323941	18.264679	-0.043292	2.249950
223.497631	1560.390219	18.269683	-0.043287	2.244972
223.416467	1552.452164	18.274688	-0.043267	2.239974
223.505962	1544.520885	18.279693	-0.043279	2.234984
223.273623	1536.563411	18.284698	-0.043230	2.229937
223.399883	1528.577047	18.289703	-0.043249	2.224892
223.201318	1520.685729	18.294707	-0.043207	2.219868
223.351286	1512.707522	18.299712	-0.043230	2.214808
223.364647	1504.753929	18.304717	-0.043228	2.209740
223.330528	1496.803038	18.309722	-0.043216	2.204657
223.265013	1488.892694	18.314727	-0.043199	2.199586
223.135970	1480.973644	18.319731	-0.043170	2.194492
223.051636	1472.983358	18.324736	-0.043149	2.189344
223.140758	1465.023844	18.329741	-0.043161	2.184220
222.872219	1457.124502	18.334746	-0.043106	2.179089
222.579720	1449.214611	18.339751	-0.043047	2.173938
222.787510	1441.220566	18.344755	-0.043080	2.168766
222.616239	1433.300613	18.349760	-0.043044	2.163594
222.702831	1425.360294	18.354765	-0.043055	2.158421
222.641226	1417.410517	18.359770	-0.043038	2.153216
222.389949	1409.482151	18.364775	-0.042987	2.147993
222.359250	1401.542115	18.369779	-0.042976	2.142772
222.646870	1393.554493	18.374784	-0.043025	2.137536
222.615813	1385.634568	18.379789	-0.043014	2.132302
222.372436	1377.709287	18.384794	-0.042964	2.127031
222.479362	1369.775453	18.389799	-0.042979	2.121775
222.390472	1361.859185	18.394803	-0.042957	2.116499
222.171374	1353.883579	18.399808	-0.042911	2.111157
222.159906	1345.928358	18.404813	-0.042904	2.105836
221.977110	1338.015242	18.409818	-0.042865	2.100513
222.001088	1330.082359	18.414823	-0.042865	2.095183
221.907681	1322.146638	18.419827	-0.042842	2.089826
221.912604	1314.201565	18.424832	-0.042838	2.084458
221.895020	1306.309203	18.429837	-0.042830	2.079110
221.725954	1298.388049	18.434842	-0.042794	2.073714
221.795474	1290.407707	18.439847	-0.042802	2.068287
221.678630	1282.499208	18.444851	-0.042775	2.062876
221.518861	1274.586374	18.449856	-0.042740	2.057444
221.471777	1266.649639	18.454861	-0.042727	2.051992
221.440179	1258.712030	18.459866	-0.042716	2.046527
221.545364	1250.766273	18.464871	-0.042730	2.041055
221.559699	1242.864090	18.469875	-0.042728	2.035590
221.476680	1234.887093	18.474880	-0.042708	2.030047
221.300262	1226.985802	18.479885	-0.042670	2.024533
221.039803	1219.098219	18.484890	-0.042616	2.019005
221.180945	1211.134055	18.489895	-0.042638	2.013449
221.091134	1203.226583	18.494899	-0.042616	2.007894
221.097233	1195.289369	18.499904	-0.042612	2.002312
220.891799	1187.414484	18.504909	-0.042569	1.996737
220.887575	1179.462851	18.509914	-0.042563	1.991112
220.882812	1171.522971	18.514919	-0.042558	1.985480
220.656763	1163.639653	18.519923	-0.042511	1.979849
220.466672	1155.737497	18.524928	-0.042470	1.974192
220.535008	1147.781173	18.529933	-0.042478	1.968508
220.463184	1139.869138	18.534938	-0.042460	1.962824
220.507462	1131.944903	18.539943	-0.042463	1.957127
220.661358	1123.974537	18.544947	-0.042487	1.951392
220.435030	1116.051137	18.549952	-0.042440	1.945633
220.473795	1108.137707	18.554957	-0.042442	1.939893
220.384781	1100.241816	18.559962	-0.042420	1.934134
220.321155	1092.308026	18.564967	-0.042404	1.928334
220.200325	1084.430380	18.569971	-0.042376	1.922551
220.004081	1076.534645	18.574976	-0.042335	1.916728
220.183082	1068.584702	18.579981	-0.042363	1.910890
219.896147	1060.694432	18.584986	-0.042305	1.905026
219.762208	1052.811981	18.589991	-0.042275	1.899166
219.888175	1044.879688	18.594995	-0.042293	1.893281
219.720219	1036.970640	18.600000	-0.042257	1.887361
219.735126	1029.069508	18.605005	-0.042255	1.881450
219.776647	1021.154435	18.610010	-0.042258	1.875512
219.596085	1013.239268	18.615015	-0.042219	1.869530
219.464556	1005.349693	18.620019	-0.042190	1.863554
219.408171	997.435356	18.625024	-0.042174	1.857548
219.656162	989.497750	18.630029	-0.042216	1.851541
219.477290	981.616180	18.635034	-0.042177	1.845507
219.305959	973.751000	18.640039	-0.042141	1.839466
219.291772	965.853718	18.645043	-0.042133	1.833400
219.016062	957.952420	18.650048	-0.042077	1.827279
219.149373	950.032299	18.655053	-0.042097	1.821172
218.996152	942.157487	18.660058	-0.042063	1.815045
218.870583	934.256636	18.665063	-0.042035	1.808880
218.831642	926.373579	18.670067	-0.042023	1.802719
218.750536	918.486413	18.675072	-0.042003	1.796528
218.907565	910.511663	18.680077	-0.042027	1.790275
218.623532	902.645303	18.685082	-0.041969	1.784033
218.295277	894.801367	18.690087	-0.041903	1.777781
218.543302	886.868922	18.695091	-0.041944	1.771507
218.433961	878.972317	18.700096	-0.041919	1.765196
218.294314	871.126453	18.705101	-0.041888	1.758898
218.168167	863.248275	18.710106	-0.041860	1.752554
218.304322	855.316695	18.715111	-0.041880	1.746176
218.187397	847.461053	18.720115	-0.041854	1.739805
217.954754	839.605579	18.725120	-0.041805	1.733395
218.097174	831.680507	18.730125	-0.041827	1.726953
217.984442	823.816919	18.735130	-0.041801	1.720505
217.785139	815.971830	18.740135	-0.041759	1.714036
217.972400	808.042300	18.745139	-0.041789	1.707523
217.815201	800.173775	18.750144	-0.041755	1.700990
217.923913	792.305767	18.755149	-0.041770	1.694468
217.685705	784.445966	18.760154	-0.041721	1.687882
217.587948	776.585482	18.765159	-0.041698	1.681288
217.474927	768.737164	18.770163	-0.041672	1.674676
217.340413	760.854632	18.775168	-0.041642	1.668006
217.365373	752.985352	18.780173	-0.041642	1.661342
217.206666	745.136121	18.785178	-0.041607	1.654643
217.068211	737.264119	18.790183	-0.041577	1.647900
217.171582	729.395297	18.795187	-0.041591	1.641166
217.348751	721.504675	18.800192	-0.041619	1.634395
217.165907	713.627848	18.805197	-0.041580	1.627558
216.976664	705.790108	18.810202	-0.041540	1.620725
217.005103	697.929955	18.815207	-0.041540	1.613874
216.804653	690.098354	18.820211	-0.041498	1.606987
216.553655	682.269805	18.825216	-0.041446	1.600065
216.792567	674.396028	18.830221	-0.041486	1.593143
216.817562	666.524394	18.835226	-0.041486	1.586162
216.460828	658.740615	18.840231	-0.041414	1.579174
216.391897	650.900451	18.845235	-0.041397	1.572146
216.432866	643.023375	18.850240	-0.041399	1.565069
216.434304	635.212852	18.855245	-0.041395	1.558014
216.055015	627.406414	18.860250	-0.041319	1.550875
216.221911	619.524148	18.865255	-0.041346	1.543714
216.101843	611.720673	18.870259	-0.041318	1.536550
215.910362	603.886209	18.875264	-0.041278	1.529312
215.898501	596.058058	18.880269	-0.041271	1.522073
215.983749	588.217561	18.885274	-0.041282	1.514803
215.756715	580.413383	18.890279	-0.041235	1.507484
215.939382	572.568942	18.895283	-0.041264	1.500154
215.899804	564.755569	18.900288	-0.041251	1.492783
215.919113	556.921623	18.905293	-0.041250	1.485365
215.784317	549.156837	18.910298	-0.041220	1.477952
215.635928	541.316296	18.915303	-0.041188	1.470427
215.462871	533.517265	18.920307	-0.041151	1.462899
215.293917	525.728820	18.925312	-0.041114	1.455343
215.188831	517.933885	18.930317	-0.041090	1.447752
215.189700	510.136422	18.935322	-0.041085	1.440134
215.061279	502.354344	18.940327	-0.041056	1.432471
215.066846	494.543112	18.945331	-0.041053	1.424759
214.785220	486.790005	18.950336	-0.040995	1.417016
214.813065	478.991182	18.955341	-0.040996	1.409236
214.612897	471.239706	18.960346	-0.040954	1.401422
214.515417	463.464752	18.965351	-0.040931	1.393558
214.734367	455.628083	18.970355	-0.040966	1.385640
214.616170	447.870192	18.975360	-0.040940	1.377700
214.510847	440.105646	18.980365	-0.040915	1.369709
214.504777	432.337030	18.985370	-0.040909	1.361684
214.120818	424.640720	18.990375	-0.040833	1.353620
213.952374	416.890039	18.995379	-0.040797	1.345490
213.970878	409.121445	19.000384	-0.040795	1.337323
213.924406	401.365410	19.005389	-0.040782	1.329109
213.752781	393.636332	19.010394	-0.040745	1.320850
213.839261	385.829165	19.015399	-0.040756	1.312501
213.952052	377.993296	19.020403	-0.040772	1.304072
213.653084	370.310963	19.025408	-0.040712	1.295681
213.467027	362.614936	19.030413	-0.040672	1.287240
213.429810	354.901604	19.035418	-0.040661	1.278753
213.456658	347.174301	19.040423	-0.040661	1.270205
213.487961	339.461534	19.045427	-0.040662	1.261616
213.306767	331.779373	19.050432	-0.040623	1.252962
213.199146	324.091314	19.055437	-0.040599	1.244256
213.114392	316.411671	19.060442	-0.040578	1.235502
213.059956	308.700414	19.065447	-0.040563	1.226655
212.842329	301.053175	19.070451	-0.040518	1.217786
212.641330	293.385723	19.075456	-0.040476	1.208831
212.763459	285.696306	19.080461	-0.040494	1.199849
212.612040	278.051487	19.085466	-0.040461	1.190796
212.668002	270.366889	19.090471	-0.040466	1.181669
212.541931	262.744195	19.095475	-0.040438	1.172507
212.337751	255.113499	19.100480	-0.040395	1.163248
212.344143	247.474435	19.105485	-0.040392	1.153948
212.040693	239.845210	19.110490	-0.040330	1.144519
211.996864	232.220919	19.115495	-0.040318	1.135073
212.007148	224.589209	19.120499	-0.040315	1.125550
211.864274	217.002847	19.125504	-0.040283	1.115970
211.606740	209.432345	19.130509	-0.040231	1.106302
211.602288	201.841666	19.135514	-0.040225	1.096579
211.539543	194.251221	19.140519	-0.040209	1.086755
211.360864	186.722399	19.145523	-0.040171	1.076897
211.287405	179.139292	19.150528	-0.040152	1.066900
211.297027	171.580417	19.155533	-0.040149	1.056860
211.356290	164.019489	19.160538	-0.040156	1.046732
210.922610	156.561684	19.165543	-0.040070	1.036530
210.925785	149.029822	19.170547	-0.040066	1.026228
210.871413	141.524567	19.175552	-0.040052	1.015845
210.657802	134.051188	19.180557	-0.040007	1.005360
210.479850	126.595286	19.185562	-0.039969	0.994798
210.309855	119.104272	19.190567	-0.039933	0.984075
210.208832	111.656799	19.195571	-0.039910	0.973314
210.115673	104.207919	19.200576	-0.039888	0.962432
210.112900	96.781155	19.205581	-0.039882	0.951482
210.057370	89.371247	19.210586	-0.039868	0.940416
209.700771	82.020528	19.215591	-0.039797	0.929228
209.789085	74.624765	19.220595	-0.039808	0.917955
209.380601	67.307580	19.225600	-0.039728	0.906527
209.255442	60.206576	19.230605	-0.039700	0.895373