Thu Mar 11 19:25:48 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.366252	-0.086085	0.000000	0.000007	0.724280

0.322333	-0.089626	0.005005	0.000015	0.724258
0.551454	-0.125435	0.010010	-0.000027	0.724268
0.581867	-0.136668	0.015014	-0.000033	0.724257
0.327012	-0.087747	0.020019	0.000014	0.724264
0.366892	-0.093372	0.025024	0.000006	0.724267
0.376995	-0.099754	0.030029	0.000004	0.724259
0.545541	-0.125017	0.035034	-0.000027	0.724269
0.627179	-0.143816	0.040038	-0.000043	0.724261
0.398065	-0.101949	0.045043	-0.000000	0.724263
0.278499	-0.078350	0.050048	0.000022	0.724268
0.303995	-0.088270	0.055053	0.000017	0.724258
0.283445	-0.079668	0.060058	0.000020	0.724268
0.172884	-0.063731	0.065062	0.000041	0.724261
0.210891	-0.071175	0.070067	0.000033	0.724260
0.537667	-0.142425	0.075072	-0.000028	0.724235
0.291223	-0.245637	0.080077	0.000018	0.723947
0.264986	-0.237380	0.085082	0.000023	0.723955
0.258629	-0.239037	0.090086	0.000024	0.723949
0.368514	-0.256847	0.095091	0.000003	0.723953
0.241006	-0.232273	0.100096	0.000027	0.723957
0.186286	-0.227112	0.105101	0.000037	0.723949
0.589887	-0.358050	0.110106	-0.000039	0.723833
0.716270	-0.485068	0.115110	-0.000062	0.723629
0.449205	-0.435726	0.120115	-0.000013	0.723633
0.618750	-0.464399	0.125120	-0.000045	0.723636
0.660545	-0.477176	0.130125	-0.000053	0.723626
0.496537	-0.555090	0.135130	-0.000022	0.723417
0.507356	-0.596031	0.140134	-0.000024	0.723341
0.549778	-0.603664	0.145139	-0.000032	0.723341
0.547488	-0.601424	0.150144	-0.000032	0.723345
0.245100	-0.667034	0.155149	0.000024	0.723111
0.239311	-0.716700	0.160154	0.000025	0.723012
0.168551	-0.707881	0.165158	0.000038	0.723005
0.229572	-0.717751	0.170163	0.000026	0.723007
0.195211	-0.837271	0.175168	0.000032	0.722761
0.374077	-0.906348	0.180173	-0.000001	0.722688
0.320735	-0.892634	0.185178	0.000009	0.722697
0.084473	-0.911813	0.190182	0.000053	0.722577
0.131360	-1.026444	0.195187	0.000044	0.722369
0.206758	-1.037643	0.200192	0.000029	0.722374
0.048256	-1.034187	0.205197	0.000059	0.722326
0.092659	-1.166301	0.210202	0.000050	0.722082
0.351613	-1.215789	0.215206	0.000002	0.722076
0.172112	-1.215776	0.220211	0.000035	0.722013
0.263274	-1.365974	0.225216	0.000018	0.721751
0.386473	-1.391844	0.230221	-0.000005	0.721743
0.246806	-1.441246	0.235226	0.000021	0.721598
0.087220	-1.493160	0.240230	0.000050	0.721440
0.138950	-1.503722	0.245235	0.000040	0.721438
0.166223	-1.642477	0.250240	0.000035	0.721175
0.196934	-1.677077	0.255245	0.000029	0.721118
0.300277	-1.737110	0.260250	0.000010	0.721037
0.134970	-1.787108	0.265254	0.000041	0.720881
-0.035147	-1.757728	0.270259	0.000072	0.720879
-0.039721	-1.925487	0.275264	0.000073	0.720548
-0.026354	-1.931794	0.280269	0.000070	0.720541
0.093603	-2.060526	0.285274	0.000048	0.720330
-0.145248	-2.071387	0.290278	0.000092	0.720225
-0.050182	-2.161045	0.295283	0.000074	0.720082
0.061959	-2.269419	0.300288	0.000053	0.719909
-0.101952	-2.291613	0.305293	0.000083	0.719808
0.121932	-2.429953	0.310298	0.000042	0.719614
0.129597	-2.476307	0.315302	0.000040	0.719526
-0.132904	-2.558509	0.320307	0.000089	0.719272
-0.749598	-2.474962	0.325312	0.000203	0.719221
-5.691060	-1.726871	0.330317	0.001123	0.718961
-4.645456	-1.909217	0.335322	0.000928	0.718969
-5.428578	-1.772355	0.340326	0.001073	0.718964
-5.525567	-1.756348	0.345331	0.001091	0.718962
-5.187750	-1.845078	0.350336	0.001028	0.718906
-6.200365	-1.797309	0.355341	0.001216	0.718645
-5.844806	-1.856801	0.360346	0.001150	0.718653
-6.471255	-1.750093	0.365350	0.001266	0.718643
-6.634024	-1.720353	0.370355	0.001297	0.718645
-6.064512	-1.818583	0.375360	0.001190	0.718652
-6.430716	-1.798006	0.380365	0.001258	0.718564
-7.283471	-1.748440	0.385370	0.001417	0.718363
-6.435584	-1.901432	0.390374	0.001259	0.718359
-7.195508	-1.767153	0.395379	0.001400	0.718357
-7.135134	-1.776365	0.400384	0.001389	0.718361
-7.130890	-1.781945	0.405389	0.001388	0.718352
-7.021198	-1.855000	0.410394	0.001367	0.718246
-8.065593	-1.783301	0.415398	0.001561	0.718021
-7.943299	-1.805835	0.420403	0.001538	0.718020
-7.941648	-1.804036	0.425408	0.001538	0.718024
-8.255405	-1.753053	0.430413	0.001596	0.718015
-8.190459	-1.761501	0.435418	0.001584	0.718022
-8.081948	-1.783318	0.440422	0.001563	0.718017
-8.376053	-1.856392	0.445427	0.001618	0.717770
-9.205586	-1.739839	0.450432	0.001772	0.717708
-9.280941	-1.731987	0.455437	0.001786	0.717698
-8.664967	-1.837201	0.460442	0.001671	0.717707
-9.173469	-1.749750	0.465446	0.001765	0.717701
-9.408708	-1.707418	0.470451	0.001809	0.717703
-8.773155	-1.818054	0.475456	0.001691	0.717708
-9.374713	-1.840018	0.480461	0.001802	0.717453
-10.229946	-1.723607	0.485466	0.001961	0.717383
-9.806333	-1.799260	0.490470	0.001882	0.717383
-9.967065	-1.771500	0.495475	0.001912	0.717381
-10.351553	-1.700215	0.500480	0.001983	0.717387
-10.430256	-1.690026	0.505485	0.001998	0.717380
-9.843608	-1.791522	0.510490	0.001888	0.717386
-10.032907	-1.813259	0.515494	0.001923	0.717277
-11.161975	-1.708943	0.520499	0.002133	0.717086
-10.318882	-1.856082	0.525504	0.001976	0.717092
-10.854421	-1.765544	0.530509	0.002076	0.717083
-11.109074	-1.716438	0.535514	0.002123	0.717091
-10.846450	-1.766612	0.540518	0.002074	0.717085
-10.700233	-1.795065	0.545523	0.002046	0.717080
-10.814359	-1.852178	0.550528	0.002068	0.716927
-12.116439	-1.709262	0.555533	0.002310	0.716752
-11.564753	-1.804064	0.560538	0.002207	0.716759
-11.553592	-1.807237	0.565542	0.002205	0.716757
-12.106458	-1.709112	0.570547	0.002307	0.716757
-11.471792	-1.817197	0.575552	0.002189	0.716767
-11.844217	-1.755592	0.580557	0.002258	0.716758
-12.262931	-1.728880	0.585562	0.002336	0.716664
-12.833647	-1.733152	0.590566	0.002442	0.716454
-12.499573	-1.794515	0.595571	0.002379	0.716451
-12.682961	-1.758381	0.600576	0.002413	0.716458
-12.960358	-1.714449	0.605581	0.002465	0.716448
-12.225079	-1.841722	0.610586	0.002328	0.716455
-12.508433	-1.794245	0.615590	0.002380	0.716450
-12.793432	-1.767878	0.620595	0.002433	0.716402
-13.421959	-1.787894	0.625600	0.002550	0.716141
-13.306455	-1.813790	0.630605	0.002528	0.716131
-13.868701	-1.708869	0.635610	0.002633	0.716141
-13.607305	-1.757208	0.640614	0.002584	0.716138
-13.567161	-1.767906	0.645619	0.002576	0.716131
-13.580454	-1.761404	0.650624	0.002578	0.716139
-13.660364	-1.750559	0.655629	0.002593	0.716133
-14.065675	-1.791654	0.660634	0.002668	0.715909
-14.338276	-1.754281	0.665638	0.002719	0.715887
-14.777235	-1.677624	0.670643	0.002800	0.715885
-14.316950	-1.756233	0.675648	0.002714	0.715892
-14.315583	-1.761481	0.680653	0.002714	0.715882
-14.357549	-1.750383	0.685658	0.002722	0.715890
-14.195850	-1.785886	0.690662	0.002691	0.715877
-14.946235	-1.817708	0.695667	0.002831	0.715549
-15.010083	-1.804132	0.700672	0.002843	0.715554
-15.704702	-1.685313	0.705677	0.002972	0.715545
-15.234006	-1.764954	0.710682	0.002884	0.715553
-15.048882	-1.799588	0.715686	0.002849	0.715551
-15.529583	-1.715059	0.720691	0.002938	0.715549
-15.009857	-1.829455	0.725696	0.002841	0.715506
-15.943574	-1.800943	0.730701	0.003015	0.715233
-16.366801	-1.721535	0.735706	0.003094	0.715241
-16.339531	-1.728245	0.740710	0.003088	0.715238
-16.096041	-1.773119	0.745715	0.003043	0.715235
-16.136332	-1.762402	0.750720	0.003050	0.715243
-16.685168	-1.669668	0.755725	0.003152	0.715233
-16.253567	-1.743529	0.760730	0.003072	0.715240
-16.421246	-1.845843	0.765734	0.003103	0.714978
-17.389550	-1.707952	0.770739	0.003283	0.714909
-17.091707	-1.756021	0.775744	0.003227	0.714920
-16.893723	-1.796289	0.780749	0.003190	0.714910
-17.491590	-1.687264	0.785754	0.003301	0.714916
-17.264842	-1.728920	0.790758	0.003259	0.714914
-17.114311	-1.757667	0.795763	0.003230	0.714910
-16.956064	-1.870684	0.800768	0.003201	0.714742
-18.427731	-1.678366	0.805773	0.003474	0.714604
-17.927268	-1.764265	0.810778	0.003381	0.714611
-17.912706	-1.765918	0.815782	0.003378	0.714613
-18.476897	-1.667569	0.820787	0.003483	0.714609
-18.124706	-1.727801	0.825792	0.003417	0.714614
-18.134532	-1.729040	0.830797	0.003419	0.714609
-18.303846	-1.731662	0.835802	0.003450	0.714544
-19.107318	-1.720097	0.840806	0.003600	0.714283
-19.168451	-1.712941	0.845811	0.003611	0.714276
-19.212314	-1.701435	0.850816	0.003619	0.714284
-19.352214	-1.680796	0.855821	0.003644	0.714276
-19.127338	-1.718898	0.860826	0.003602	0.714280
-18.811261	-1.776194	0.865830	0.003543	0.714279
-19.039901	-1.735934	0.870835	0.003586	0.714278
-19.099053	-1.797689	0.875840	0.003597	0.714135
-20.153933	-1.695419	0.880845	0.003793	0.713965
-19.699443	-1.772822	0.885850	0.003708	0.713972
-19.869439	-1.743362	0.890854	0.003739	0.713971
-20.170451	-1.692013	0.895859	0.003795	0.713967
-19.720737	-1.766797	0.900864	0.003711	0.713978
-20.100656	-1.704964	0.905869	0.003782	0.713967
-20.074673	-1.757585	0.910874	0.003777	0.713872
-20.906785	-1.718170	0.915878	0.003931	0.713656
-20.882215	-1.725416	0.920883	0.003927	0.713651
-21.003928	-1.699690	0.925888	0.003949	0.713659
-20.792786	-1.743553	0.930893	0.003910	0.713647
-20.622124	-1.769566	0.935898	0.003878	0.713656
-21.068251	-1.691418	0.940902	0.003960	0.713654
-21.129169	-1.683001	0.945907	0.003972	0.713649
-21.111547	-1.807462	0.950912	0.003968	0.713409
-21.953195	-1.682112	0.955917	0.004125	0.713360
-21.829531	-1.702226	0.960922	0.004101	0.713364
-21.367672	-1.784244	0.965926	0.004015	0.713365
-21.882637	-1.696889	0.970931	0.004111	0.713357
-22.096404	-1.653430	0.975936	0.004150	0.713368
-22.082999	-1.660412	0.980941	0.004148	0.713359
-21.747479	-1.808746	0.985946	0.004085	0.713183
-22.890475	-1.684448	0.990950	0.004298	0.713026
-22.676936	-1.722773	0.995955	0.004258	0.713026
-22.487854	-1.753328	1.000960	0.004222	0.713032
-22.952110	-1.675162	1.005965	0.004309	0.713024
-23.015452	-1.659957	1.010970	0.004320	0.713032
-22.662188	-1.724432	1.015974	0.004254	0.713029
-22.748736	-1.746271	1.020979	0.004270	0.712956
-23.339282	-1.757818	1.025984	0.004380	0.712723
-23.290558	-1.771285	1.030989	0.004371	0.712714
-23.486358	-1.734872	1.035994	0.004407	0.712718
-23.573645	-1.719557	1.040998	0.004423	0.712718
-23.772566	-1.686783	1.046003	0.004460	0.712713
-23.436839	-1.741744	1.051008	0.004397	0.712723
-23.819998	-1.711422	1.056013	0.004468	0.712648
-24.529398	-1.711688	1.061018	0.004600	0.712396
-24.098310	-1.788974	1.066022	0.004520	0.712395
-24.594615	-1.703561	1.071027	0.004612	0.712390
-24.612445	-1.696508	1.076032	0.004615	0.712398
-24.867962	-1.656742	1.081037	0.004662	0.712387
-24.717748	-1.680885	1.086042	0.004634	0.712392
-24.312844	-1.753662	1.091046	0.004558	0.712391
-25.023961	-1.744604	1.096051	0.004691	0.712157
-25.186849	-1.743862	1.101056	0.004721	0.712101
-25.463032	-1.698844	1.106061	0.004772	0.712094
-25.573746	-1.677318	1.111066	0.004792	0.712097
-25.205387	-1.743936	1.116070	0.004724	0.712096
-25.384356	-1.715575	1.121075	0.004757	0.712089
-25.206332	-1.741542	1.126080	0.004723	0.712101
-25.723101	-1.777162	1.131085	0.004819	0.711847
-26.208845	-1.731170	1.136090	0.004910	0.711767
-26.094484	-1.750455	1.141094	0.004888	0.711769
-26.663531	-1.653327	1.146099	0.004994	0.711761
-26.099212	-1.749933	1.151104	0.004889	0.711769
-26.101586	-1.754524	1.156109	0.004889	0.711760
-26.242080	-1.725812	1.161114	0.004915	0.711767
-26.391155	-1.811274	1.166118	0.004942	0.711544
-27.195285	-1.714318	1.171123	0.005092	0.711452
-27.049585	-1.735198	1.176128	0.005064	0.711463
-27.162939	-1.720324	1.181133	0.005085	0.711453
-27.248760	-1.703039	1.186138	0.005101	0.711457
-26.878005	-1.769187	1.191142	0.005032	0.711457
-27.278485	-1.699431	1.196147	0.005106	0.711455
-27.138626	-1.837501	1.201152	0.005080	0.711229
-28.141676	-1.703470	1.206157	0.005267	0.711140
-28.331861	-1.668605	1.211162	0.005302	0.711143
-27.899067	-1.745576	1.216166	0.005221	0.711143
-28.186146	-1.696730	1.221171	0.005274	0.711139
-28.101238	-1.707757	1.226176	0.005258	0.711148
-28.459273	-1.649943	1.231181	0.005325	0.711136
-28.204349	-1.742929	1.236186	0.005277	0.711042
-28.819094	-1.714597	1.241190	0.005391	0.710880
-29.054703	-1.677111	1.246195	0.005435	0.710871
-28.842694	-1.710399	1.251200	0.005395	0.710881
-28.780654	-1.726110	1.256205	0.005383	0.710872
-28.989196	-1.688756	1.261210	0.005422	0.710873
-28.817285	-1.717948	1.266214	0.005390	0.710876
-28.978872	-1.759522	1.271219	0.005420	0.710736
-29.647585	-1.737790	1.276224	0.005544	0.710542
-29.595249	-1.752318	1.281229	0.005534	0.710532
-29.655440	-1.740305	1.286234	0.005545	0.710535
-29.675494	-1.734977	1.291238	0.005549	0.710539
-30.147431	-1.656154	1.296243	0.005636	0.710528
-29.812801	-1.710124	1.301248	0.005574	0.710540
-29.918338	-1.756963	1.306253	0.005593	0.710409
-30.928877	-1.669617	1.311258	0.005781	0.710224
-30.365421	-1.770464	1.316262	0.005676	0.710224
-30.587159	-1.735287	1.321267	0.005717	0.710216
-30.585597	-1.728734	1.326272	0.005717	0.710230
-30.885736	-1.680914	1.331277	0.005772	0.710219
-31.002460	-1.657382	1.336282	0.005794	0.710225
-30.679212	-1.768498	1.341286	0.005733	0.710118
-32.154260	-1.618784	1.346291	0.006008	0.709892
-31.617084	-1.710382	1.351296	0.005908	0.709901
-31.642310	-1.710223	1.356301	0.005912	0.709893
-31.769727	-1.687520	1.361306	0.005936	0.709893
-31.593143	-1.717510	1.366310	0.005903	0.709896
-31.836298	-1.676835	1.371315	0.005948	0.709892
-31.484313	-1.735078	1.376320	0.005882	0.709901
-32.041730	-1.748665	1.381325	0.005985	0.709676
-32.669881	-1.674692	1.386330	0.006102	0.709600
-32.163483	-1.763033	1.391334	0.006008	0.709604
-32.449925	-1.716359	1.396339	0.006061	0.709596
-32.682859	-1.670128	1.401344	0.006104	0.709606
-32.394897	-1.725393	1.406349	0.006050	0.709598
-32.287170	-1.743854	1.411354	0.006030	0.709600
-32.690393	-1.813892	1.416358	0.006105	0.709317
-33.685785	-1.664345	1.421363	0.006290	0.709261
-33.439403	-1.703502	1.426368	0.006244	0.709271
-33.486239	-1.697967	1.431373	0.006252	0.709266
-33.521577	-1.690659	1.436378	0.006259	0.709268
-33.026843	-1.776144	1.441382	0.006166	0.709274
-33.414220	-1.712101	1.446387	0.006238	0.709265
-33.799062	-1.761404	1.451392	0.006310	0.709029
-34.593031	-1.653900	1.456397	0.006457	0.708961
-34.416984	-1.686995	1.461402	0.006424	0.708958
-34.269797	-1.712686	1.466406	0.006397	0.708960
-34.524673	-1.671007	1.471411	0.006444	0.708953
-33.998042	-1.759569	1.476416	0.006346	0.708964
-34.193366	-1.729011	1.481421	0.006382	0.708956
-34.635286	-1.735620	1.486426	0.006464	0.708785
-35.209725	-1.704248	1.491430	0.006571	0.708643
-35.183805	-1.711912	1.496435	0.006566	0.708637
-35.319920	-1.683370	1.501440	0.006591	0.708646
-35.033383	-1.738262	1.506445	0.006537	0.708639
-34.925306	-1.756828	1.511450	0.006517	0.708641
-35.114250	-1.719961	1.516454	0.006552	0.708648
-35.396915	-1.742136	1.521459	0.006604	0.708503
-35.788319	-1.745576	1.526464	0.006677	0.708357
-35.861149	-1.736611	1.531469	0.006690	0.708349
-36.342113	-1.649957	1.536474	0.006780	0.708351
-35.859835	-1.735102	1.541478	0.006690	0.708353
-35.766889	-1.754866	1.546483	0.006672	0.708347
-36.176768	-1.677337	1.551488	0.006748	0.708357
-36.204416	-1.784456	1.556493	0.006753	0.708132
-37.140058	-1.676408	1.561498	0.006927	0.708015
-36.949423	-1.709067	1.566502	0.006892	0.708018
-36.790940	-1.741913	1.571507	0.006862	0.708009
-36.523487	-1.785072	1.576512	0.006812	0.708019
-36.744844	-1.749243	1.581517	0.006853	0.708012
-36.950948	-1.711577	1.586522	0.006891	0.708014
-36.861700	-1.851891	1.591526	0.006874	0.707765
-37.748109	-1.729859	1.596531	0.007039	0.707693
-37.989248	-1.681279	1.601536	0.007084	0.707705
-37.786617	-1.721603	1.606541	0.007046	0.707697
-37.727859	-1.731458	1.611546	0.007035	0.707699
-37.815245	-1.712268	1.616550	0.007051	0.707706
-37.995867	-1.685020	1.621555	0.007084	0.707697
-37.942821	-1.808903	1.626560	0.007074	0.707468
-38.837292	-1.695488	1.631565	0.007240	0.707376
-38.721049	-1.716290	1.636570	0.007219	0.707376
-38.588029	-1.738099	1.641574	0.007194	0.707380
-38.927497	-1.681057	1.646579	0.007257	0.707374
-39.005411	-1.663518	1.651584	0.007271	0.707381
-38.877342	-1.689189	1.656589	0.007247	0.707376
-38.885803	-1.736417	1.661594	0.007248	0.707279
-39.542282	-1.714436	1.666598	0.007370	0.707088
-39.799113	-1.670760	1.671603	0.007418	0.707084
-39.518716	-1.717597	1.676608	0.007365	0.707091
-39.604836	-1.706449	1.681613	0.007381	0.707083
-39.809479	-1.669510	1.686618	0.007419	0.707084
-39.573053	-1.709558	1.691622	0.007375	0.707089
-39.610632	-1.719814	1.696627	0.007382	0.707055
-40.385913	-1.730098	1.701632	0.007526	0.706758
-40.381093	-1.733759	1.706637	0.007525	0.706752
-40.673876	-1.681186	1.711642	0.007579	0.706753
-40.094939	-1.782329	1.716646	0.007471	0.706758
-40.615334	-1.694895	1.721651	0.007568	0.706748
-40.635907	-1.684510	1.726656	0.007571	0.706762
-40.322783	-1.760536	1.731661	0.007513	0.706721
-41.341889	-1.717337	1.736666	0.007702	0.706444
-41.113419	-1.756010	1.741670	0.007660	0.706448
-41.583145	-1.677526	1.746675	0.007747	0.706438
-41.453895	-1.696648	1.751680	0.007723	0.706446
-41.403164	-1.709114	1.756685	0.007713	0.706440
-41.299198	-1.729011	1.761690	0.007693	0.706437
-40.900650	-1.816916	1.766694	0.007619	0.706404
-42.462748	-1.677592	1.771699	0.007910	0.706125
-42.108242	-1.735667	1.776704	0.007843	0.706135
-41.922744	-1.774213	1.781709	0.007809	0.706125
-42.246089	-1.715724	1.786714	0.007869	0.706127
-42.017559	-1.753905	1.791718	0.007826	0.706132
-42.207539	-1.724120	1.796723	0.007861	0.706125
-42.309633	-1.730732	1.801728	0.007880	0.706075
-43.202671	-1.678627	1.806733	0.008046	0.705860
-42.914957	-1.728447	1.811738	0.007992	0.705864
-42.933615	-1.723418	1.816742	0.007995	0.705867
-43.356634	-1.653098	1.821747	0.008074	0.705858
-42.779138	-1.751160	1.826752	0.007966	0.705868
-42.721439	-1.766224	1.831757	0.007955	0.705859
-43.259545	-1.733980	1.836762	0.008055	0.705731
-44.036505	-1.694985	1.841766	0.008200	0.705531
-43.684631	-1.763381	1.846771	0.008134	0.705520
-43.851752	-1.730258	1.851776	0.008165	0.705527
-44.107534	-1.684937	1.856781	0.008212	0.705527
-43.920587	-1.718424	1.861786	0.008177	0.705527
-43.630688	-1.768402	1.866790	0.008123	0.705531
-44.211632	-1.742644	1.871795	0.008231	0.705375
-45.044301	-1.672261	1.876800	0.008386	0.705218
-44.358442	-1.797598	1.881805	0.008258	0.705212
-44.885582	-1.702854	1.886810	0.008356	0.705214
-44.878187	-1.702317	1.891814	0.008354	0.705218
-44.538829	-1.766270	1.896819	0.008291	0.705212
-44.580624	-1.753552	1.901824	0.008299	0.705223
-45.090227	-1.766830	1.906829	0.008393	0.705014
-45.954388	-1.674513	1.911834	0.008554	0.704890
-45.256865	-1.792941	1.916838	0.008424	0.704902
-45.737503	-1.712492	1.921843	0.008513	0.704892
-45.623109	-1.729054	1.926848	0.008492	0.704900
-45.278593	-1.793927	1.931853	0.008427	0.704893
-45.902351	-1.684127	1.936858	0.008543	0.704891
-46.214072	-1.726276	1.941862	0.008601	0.704694
-46.734754	-1.684935	1.946867	0.008698	0.704591
-46.225303	-1.770769	1.951872	0.008603	0.704602
-46.490170	-1.727234	1.956877	0.008652	0.704595
-46.662658	-1.696798	1.961882	0.008684	0.704594
-46.305960	-1.756948	1.966886	0.008617	0.704602
-46.735093	-1.684592	1.971891	0.008697	0.704594
-47.027205	-1.734220	1.976896	0.008751	0.704389
-47.564781	-1.699909	1.981901	0.008851	0.704265
-47.346521	-1.738749	1.986906	0.008810	0.704266
-47.221940	-1.757016	1.991910	0.008787	0.704274
-47.696657	-1.679163	1.996915	0.008875	0.704261
-47.392687	-1.729162	2.001920	0.008818	0.704270

-47.628951	-1.740735	2.011917	0.008862	0.704163
-48.453482	-1.695857	2.021914	0.009015	0.703957
-48.138065	-1.752722	2.031910	0.008956	0.703957
-48.557221	-1.679048	2.041907	0.009033	0.703956
-48.318689	-1.721237	2.051904	0.008988	0.703957
-48.545668	-1.679888	2.061901	0.009030	0.703960
-48.547171	-1.681839	2.071898	0.009030	0.703956
-47.781268	-1.687022	2.081894	0.008887	0.704222
-47.578559	-1.702821	2.091891	0.008849	0.704263
-47.329570	-1.747105	2.101888	0.008802	0.704264
-47.584940	-1.701587	2.111885	0.008849	0.704265
-47.445855	-1.727363	2.121882	0.008823	0.704264
-47.506629	-1.717972	2.131878	0.008834	0.704262
-47.648163	-1.692129	2.141875	0.008860	0.704264
-47.696354	-1.680252	2.151872	0.008868	0.704271
-47.007056	-1.642859	2.161869	0.008740	0.704595
-46.840003	-1.674707	2.171866	0.008708	0.704592
-46.578449	-1.720726	2.181862	0.008659	0.704594
-46.662327	-1.705588	2.191859	0.008674	0.704595
-46.235577	-1.695684	2.201856	0.008594	0.704769
-45.715938	-1.727421	2.211853	0.008497	0.704893
-45.772912	-1.717778	2.221850	0.008507	0.704892
-46.003448	-1.678706	2.231846	0.008550	0.704889
-45.685495	-1.647854	2.241843	0.008490	0.705066
-45.086940	-1.680006	2.251840	0.008378	0.705217
-45.258047	-1.649396	2.261837	0.008410	0.705218
-44.841974	-1.725520	2.271834	0.008332	0.705215
-44.347156	-1.670234	2.281830	0.008239	0.705505
-44.225083	-1.679888	2.291827	0.008216	0.705530
-43.973745	-1.724275	2.301824	0.008169	0.705531
-44.139461	-1.657418	2.311821	0.008199	0.705607
-43.255440	-1.685765	2.321818	0.008034	0.705868
-43.234908	-1.691650	2.331814	0.008030	0.705864
-43.296706	-1.679943	2.341811	0.008041	0.705867
-42.678858	-1.705062	2.351808	0.007926	0.706038
-42.502430	-1.691277	2.361805	0.007893	0.706130
-42.337976	-1.720563	2.371802	0.007861	0.706131
-42.507995	-1.678602	2.381798	0.007893	0.706155
-41.817845	-1.656062	2.391795	0.007764	0.706449
-41.348339	-1.741086	2.401792	0.007676	0.706447
-41.701449	-1.676945	2.411789	0.007741	0.706450
-41.030894	-1.698582	2.421786	0.007616	0.706647
-40.848251	-1.678236	2.431782	0.007582	0.706755
-40.595059	-1.724077	2.441779	0.007534	0.706754
-40.758275	-1.664020	2.451776	0.007564	0.706817
-39.848537	-1.693475	2.461773	0.007394	0.707084
-39.743156	-1.712929	2.471770	0.007374	0.707084
-40.105957	-1.649203	2.481766	0.007441	0.707083
-39.395435	-1.666925	2.491763	0.007309	0.707302
-38.899285	-1.716973	2.501760	0.007216	0.707380
-39.186165	-1.666274	2.511757	0.007269	0.707380
-38.891069	-1.657189	2.521754	0.007213	0.707504
-38.065784	-1.708308	2.531750	0.007059	0.707698
-38.060831	-1.707368	2.541747	0.007058	0.707702
-38.067367	-1.705353	2.551744	0.007059	0.707705
-37.481762	-1.680981	2.561741	0.006949	0.707964
-37.360953	-1.678744	2.571738	0.006926	0.708012
-37.495863	-1.654979	2.581734	0.006951	0.708012
-37.023783	-1.660301	2.591731	0.006863	0.708171
-36.418329	-1.678221	2.601728	0.006750	0.708352
-36.513271	-1.662867	2.611725	0.006767	0.708350
-36.251130	-1.706944	2.621722	0.006718	0.708356
-35.745465	-1.655593	2.631718	0.006623	0.708640
-35.583506	-1.683179	2.641715	0.006593	0.708644
-35.629047	-1.675187	2.651712	0.006601	0.708644
-35.180366	-1.652453	2.661709	0.006517	0.708851
-34.762593	-1.673484	2.671706	0.006438	0.708958
-35.010482	-1.630443	2.681702	0.006484	0.708957
-34.540859	-1.667421	2.691699	0.006396	0.709051
-33.996055	-1.654959	2.701696	0.006294	0.709271
-34.017087	-1.652155	2.711693	0.006298	0.709270
-33.862290	-1.680375	2.721690	0.006269	0.709270
-33.222105	-1.635688	2.731686	0.006149	0.709588
-32.789529	-1.706927	2.741683	0.006068	0.709601
-32.889941	-1.689351	2.751680	0.006086	0.709601
-32.862009	-1.643499	2.761677	0.006081	0.709703
-32.164714	-1.671629	2.771674	0.005951	0.709896
-32.306674	-1.647626	2.781670	0.005977	0.709895
-31.922158	-1.716159	2.791667	0.005905	0.709895
-31.482103	-1.644062	2.801664	0.005822	0.710197
-31.314979	-1.663136	2.811661	0.005791	0.710219
-31.404355	-1.648466	2.821658	0.005807	0.710217
-31.030648	-1.631213	2.831654	0.005737	0.710386
-30.178725	-1.709176	2.841651	0.005578	0.710534
-30.302011	-1.686234	2.851648	0.005600	0.710537
-30.121592	-1.719331	2.861645	0.005566	0.710536
-29.969860	-1.598761	2.871642	0.005538	0.710831
-29.431798	-1.676801	2.881638	0.005437	0.710868
-29.330540	-1.693129	2.891635	0.005418	0.710872
-29.312829	-1.642188	2.901632	0.005414	0.710981
-28.632611	-1.683451	2.911629	0.005287	0.711141
-28.834159	-1.648716	2.921626	0.005324	0.711140
-28.893613	-1.621875	2.931622	0.005335	0.711173
-27.684283	-1.695580	2.941619	0.005109	0.711456
-27.786541	-1.678265	2.951616	0.005128	0.711455
-27.781220	-1.680081	2.961613	0.005126	0.711454
-27.490615	-1.631165	2.971610	0.005072	0.711656
-26.771871	-1.706137	2.981606	0.004938	0.711763
-27.057551	-1.655864	2.991603	0.004990	0.711762
-26.987804	-1.630745	3.001600	0.004977	0.711838
-25.798031	-1.716267	3.011597	0.004755	0.712091
-26.191428	-1.645272	3.021594	0.004828	0.712093
-26.064425	-1.669045	3.031590	0.004804	0.712092
-25.559880	-1.652740	3.041587	0.004710	0.712304
-25.312654	-1.654506	3.051584	0.004663	0.712389
-25.237855	-1.667486	3.061581	0.004649	0.712391
-25.348978	-1.587816	3.071578	0.004669	0.712511
-24.145647	-1.703292	3.081574	0.004445	0.712709
-24.460534	-1.647073	3.091571	0.004503	0.712710
-24.311082	-1.672726	3.101568	0.004475	0.712712
-23.422738	-1.689992	3.111565	0.004309	0.712994
-23.606341	-1.643028	3.121562	0.004342	0.713023
-23.226050	-1.712401	3.131558	0.004271	0.713021
-23.465816	-1.621970	3.141555	0.004315	0.713116
-22.426178	-1.687596	3.151552	0.004121	0.713355
-22.609717	-1.653838	3.161549	0.004155	0.713358
-22.485468	-1.675902	3.171546	0.004132	0.713359
-21.842093	-1.675832	3.181542	0.004011	0.713588
-21.740802	-1.662518	3.191539	0.003992	0.713651
-21.456867	-1.714329	3.201536	0.003939	0.713649
-21.745364	-1.627202	3.211533	0.003992	0.713721
-20.832207	-1.666128	3.221530	0.003822	0.713968
-20.695918	-1.691672	3.231526	0.003796	0.713966
-20.899367	-1.654329	3.241523	0.003833	0.713969
-20.049066	-1.695265	3.251520	0.003675	0.714190
-20.139556	-1.634182	3.261517	0.003691	0.714280
-19.928349	-1.672641	3.271514	0.003651	0.714279
-19.785683	-1.661432	3.281510	0.003624	0.714352
-18.929727	-1.684771	3.291507	0.003465	0.714610
-18.740824	-1.717444	3.301504	0.003429	0.714612
-19.203639	-1.635625	3.311501	0.003515	0.714612
-18.505021	-1.668445	3.321498	0.003384	0.714795
-18.018944	-1.697950	3.331494	0.003293	0.714909
-18.301882	-1.646445	3.341491	0.003346	0.714912
-17.952292	-1.692032	3.351488	0.003280	0.714946
-17.444482	-1.637589	3.361485	0.003185	0.715234
-17.058265	-1.706277	3.371482	0.003113	0.715235
-17.318681	-1.662331	3.381478	0.003161	0.715231
-16.809408	-1.665113	3.391475	0.003066	0.715406
-16.079667	-1.723584	3.401472	0.002929	0.715549
-16.469235	-1.654464	3.411469	0.003001	0.715549
-16.172751	-1.708112	3.421466	0.002946	0.715548
-15.654155	-1.644298	3.431462	0.002849	0.715859
-15.550858	-1.651464	3.441459	0.002829	0.715882
-15.369500	-1.682748	3.451456	0.002795	0.715884
-15.485166	-1.599755	3.461453	0.002816	0.716009
-14.663745	-1.684824	3.471450	0.002663	0.716131
-14.970008	-1.630744	3.481446	0.002719	0.716131
-14.581767	-1.662309	3.491443	0.002647	0.716206
-13.736727	-1.690593	3.501440	0.002489	0.716449
-13.808656	-1.678493	3.511437	0.002502	0.716448
-13.717950	-1.694140	3.521434	0.002485	0.716450
-13.356464	-1.639835	3.531430	0.002417	0.716686
-13.235871	-1.625270	3.541427	0.002394	0.716758
-12.916461	-1.681853	3.551424	0.002334	0.716760
-12.448254	-1.696702	3.561421	0.002247	0.716896
-11.370801	-1.793748	3.571418	0.002046	0.717084
-11.696130	-1.734419	3.581414	0.002106	0.717088
-11.305401	-1.804454	3.591411	0.002033	0.717088
-11.746085	-1.709763	3.601408	0.002114	0.717121
-10.867282	-1.734558	3.611405	0.001950	0.717382
-10.500738	-1.799809	3.621402	0.001882	0.717383
-10.693905	-1.766669	3.631398	0.001917	0.717381
-10.680279	-1.747479	3.641395	0.001914	0.717425
-9.649229	-1.787389	3.651392	0.001722	0.717710
-9.639337	-1.788994	3.661389	0.001719	0.717711
-9.849857	-1.752962	3.671386	0.001758	0.717709
-9.904699	-1.704325	3.681382	0.001768	0.717786
-8.612313	-1.816574	3.691379	0.001527	0.718020
-8.591245	-1.818548	3.701376	0.001523	0.718024
-8.752835	-1.790560	3.711373	0.001552	0.718024
-8.612387	-1.748715	3.721370	0.001526	0.718156
-7.885363	-1.776821	3.731366	0.001390	0.718357
-7.662840	-1.814833	3.741363	0.001348	0.718361
-7.805633	-1.789917	3.751360	0.001374	0.718361
-7.369251	-1.799282	3.761357	0.001293	0.718497
-6.844990	-1.816206	3.771354	0.001195	0.718649
-7.132070	-1.765830	3.781350	0.001248	0.718648
-7.022408	-1.785600	3.791347	0.001227	0.718648
-6.451243	-1.748993	3.801344	0.001120	0.718922
-5.988628	-1.811065	3.811341	0.001033	0.718963
-5.929671	-1.821923	3.821338	0.001022	0.718963
-5.970073	-1.791752	3.831334	0.001029	0.719009
-4.976146	-1.835078	3.841331	0.000844	0.719274
-5.225669	-1.789926	3.851328	0.000890	0.719276
-5.285410	-1.778574	3.861325	0.000900	0.719278
-4.821953	-1.756471	3.871322	0.000814	0.719485
-4.120898	-1.820942	3.881318	0.000683	0.719605
-4.174164	-1.811655	3.891315	0.000692	0.719605
-4.200933	-1.807483	3.901312	0.000697	0.719605
-3.298060	-1.833517	3.911309	0.000528	0.719871
-3.383896	-1.803356	3.921306	0.000544	0.719901
-3.201105	-1.834719	3.931302	0.000509	0.719904
-3.102465	-1.838323	3.941299	0.000491	0.719933
-2.490288	-1.796129	3.951296	0.000376	0.720231
-2.467379	-1.800328	3.961293	0.000372	0.720232
-2.434832	-1.808784	3.971290	0.000365	0.720227
-2.095543	-1.788275	3.981286	0.000302	0.720387
-1.716548	-1.775175	3.991283	0.000231	0.720547
-1.582532	-1.799001	4.001280	0.000205	0.720548
-1.560839	-1.784600	4.011277	0.000201	0.720584
-1.265153	-1.683912	4.021274	0.000145	0.720887
-1.121476	-1.709101	4.031270	0.000118	0.720889
-1.058619	-1.707542	4.041267	0.000106	0.720914
-1.393920	-1.537856	4.051264	0.000168	0.721132
-1.162608	-1.579205	4.061261	0.000124	0.721132
-1.239414	-1.440213	4.071258	0.000138	0.721379
-1.089254	-1.435467	4.081254	0.000110	0.721442
-0.892400	-1.356644	4.091251	0.000073	0.721666
-0.840506	-1.323489	4.101248	0.000063	0.721751
-0.813680	-1.195482	4.111245	0.000057	0.722012
-0.898560	-1.138549	4.121242	0.000072	0.722095
-0.530567	-1.063781	4.131238	0.000003	0.722371
-0.583479	-0.995002	4.141235	0.000013	0.722489
-0.629528	-0.880844	4.151232	0.000021	0.722697
-0.452254	-0.781201	4.161229	-0.000013	0.722956
-0.336020	-0.716390	4.171226	-0.000035	0.723124
-0.434587	-0.587327	4.181222	-0.000017	0.723344
-0.316764	-0.467409	4.191219	-0.000039	0.723621
-0.343938	-0.352176	4.201216	-0.000035	0.723838
-0.164338	-0.265824	4.211213	-0.000069	0.724070
-0.258454	-0.124116	4.221210	-0.000052	0.724316
-0.307221	0.027569	4.231206	-0.000043	0.724596
0.000000	0.167316	4.241203	-0.000101	0.724978

0.111567	0.752713	4.246208	-0.000122	0.726161
0.025916	2.045431	4.251213	-0.000107	0.728652
0.308139	3.863883	4.256218	-0.000161	0.732280
0.534284	6.247409	4.261222	-0.000205	0.736960
0.641101	9.159293	4.266227	-0.000227	0.742579
1.104675	12.488925	4.271232	-0.000316	0.749067
1.470862	16.295332	4.276237	-0.000387	0.756361
1.743179	20.518119	4.281242	-0.000440	0.764327
2.022589	25.143493	4.286246	-0.000496	0.772953
2.688361	30.065017	4.291251	-0.000623	0.782144
2.912999	35.412217	4.296256	-0.000668	0.791851
3.129583	41.078852	4.301261	-0.000713	0.802003
3.560665	47.004746	4.306266	-0.000797	0.812547
4.080693	53.200171	4.311270	-0.000898	0.823446
4.403627	59.707680	4.316275	-0.000963	0.834675
4.777703	66.402194	4.321280	-0.001037	0.846082
5.434035	73.298566	4.326285	-0.001164	0.857754
5.824336	80.435145	4.331290	-0.001241	0.869584
6.225187	87.753914	4.336294	-0.001321	0.881551
6.875006	95.213166	4.341299	-0.001447	0.893649
7.386747	102.848205	4.346304	-0.001547	0.905823
7.785795	110.657762	4.351309	-0.001627	0.918075
9.413902	118.348251	4.356314	-0.001935	0.930311
10.935373	126.210706	4.361318	-0.002224	0.942618
11.708326	134.319817	4.366323	-0.002373	0.954938
12.421323	142.505870	4.371328	-0.002512	0.967197
13.490951	150.745500	4.376333	-0.002717	0.979471
14.293882	159.111794	4.381338	-0.002872	0.991706
14.689893	167.580138	4.386342	-0.002951	1.003836
15.408291	176.040397	4.391347	-0.003091	1.015888
16.195614	184.512405	4.396352	-0.003243	1.027831
16.972501	193.043956	4.401357	-0.003393	1.039714
17.602047	201.619166	4.406362	-0.003516	1.051488
18.379009	210.197758	4.411366	-0.003667	1.063169
19.013414	218.845372	4.416371	-0.003791	1.074782
19.591001	227.471331	4.421376	-0.003904	1.086229
20.132369	236.137600	4.426381	-0.004011	1.097600
20.917246	244.750918	4.431386	-0.004163	1.108840
21.456918	253.419806	4.436390	-0.004269	1.119984
22.369952	262.024341	4.441395	-0.004445	1.131017
23.310378	270.607840	4.446400	-0.004626	1.141923
23.921449	279.294030	4.451405	-0.004746	1.152783
24.569578	287.915557	4.456410	-0.004872	1.163469
25.491049	296.492385	4.461414	-0.005049	1.174061
26.213578	305.093388	4.466419	-0.005190	1.184545
26.559333	313.751169	4.471424	-0.005260	1.194929
27.442969	322.296885	4.476429	-0.005430	1.205198
28.126204	330.879901	4.481434	-0.005563	1.215384
28.693164	339.462011	4.486438	-0.005675	1.225462
29.172029	348.073126	4.491443	-0.005770	1.235473
29.772419	356.586848	4.496448	-0.005887	1.245315
30.341853	365.133094	4.501453	-0.005999	1.255112
30.771763	373.668257	4.506458	-0.006085	1.264793
31.918255	382.092856	4.511462	-0.006304	1.274412
32.468656	390.600499	4.516467	-0.006412	1.283939
32.609252	399.160964	4.521472	-0.006444	1.293378
33.272469	407.625927	4.526477	-0.006573	1.302740
33.656440	416.203672	4.531482	-0.006651	1.312106
34.219191	424.669116	4.536486	-0.006761	1.321318
34.780234	433.080790	4.541491	-0.006871	1.330407
35.111700	441.508695	4.546496	-0.006939	1.339412
35.764876	449.882074	4.551501	-0.007066	1.348355
36.340804	458.264510	4.556506	-0.007179	1.357235
36.720885	466.649243	4.561510	-0.007255	1.366026
37.091956	475.067918	4.566515	-0.007330	1.374793
37.462193	483.437498	4.571520	-0.007405	1.383455
37.891816	491.829476	4.576525	-0.007491	1.392095
38.691864	500.112751	4.581530	-0.007645	1.400634
39.064042	508.469628	4.586534	-0.007720	1.409124
39.652396	516.805078	4.591539	-0.007835	1.417577
40.225708	525.100212	4.596544	-0.007948	1.425937
40.784505	533.438786	4.601549	-0.008057	1.434289
40.948771	541.798230	4.606554	-0.008094	1.442548
41.182818	550.139271	4.611558	-0.008143	1.450754
42.027090	558.382777	4.616563	-0.008306	1.458917
42.390287	566.689774	4.621568	-0.008379	1.467018
43.015140	575.026525	4.626573	-0.008501	1.475145
43.666595	583.260014	4.631578	-0.008628	1.483132
43.947751	591.567025	4.636582	-0.008686	1.491089
44.364406	599.858720	4.641587	-0.008769	1.499010
45.062041	608.069989	4.646592	-0.008904	1.506856
45.471909	616.377262	4.651597	-0.008986	1.514708
45.900177	624.625907	4.656602	-0.009072	1.522467
46.367600	632.879506	4.661606	-0.009164	1.530197
46.785011	641.160224	4.666611	-0.009248	1.537906
47.131006	649.404038	4.671616	-0.009318	1.545531
47.549830	657.688044	4.676621	-0.009401	1.553167
48.111201	665.882648	4.681626	-0.009511	1.560704
48.505721	674.119329	4.686630	-0.009590	1.568219
49.066803	682.340169	4.691635	-0.009700	1.575708
49.546706	690.549017	4.696640	-0.009795	1.583138
49.998781	698.784704	4.701645	-0.009885	1.590554
50.175970	707.056058	4.706650	-0.009924	1.597928
50.573578	715.248745	4.711654	-0.010003	1.605229
51.172805	723.461305	4.716659	-0.010120	1.612543
51.544687	731.665821	4.721664	-0.010195	1.619785
52.124634	739.861151	4.726669	-0.010309	1.627016
52.602845	748.125750	4.731674	-0.010403	1.634260
53.109889	756.294547	4.736678	-0.010503	1.641393
53.646412	764.472623	4.741683	-0.010609	1.648508
53.912766	772.695547	4.746688	-0.010664	1.655593
54.371360	780.870691	4.751693	-0.010755	1.662633
54.728242	789.067365	4.756698	-0.010827	1.669648
54.851054	797.301873	4.761702	-0.010855	1.676634
55.672587	805.411425	4.766707	-0.011014	1.683579
56.193239	813.575209	4.771712	-0.011116	1.690501
56.318692	821.822385	4.776717	-0.011145	1.697412
56.587068	830.009970	4.781722	-0.011201	1.704264
57.006474	838.198917	4.786726	-0.011284	1.711109
57.533678	846.367426	4.791731	-0.011388	1.717924
57.744651	854.525883	4.796736	-0.011433	1.724663
58.082885	862.713705	4.801741	-0.011501	1.731416
58.427740	870.884935	4.806746	-0.011571	1.738130
58.892107	879.019997	4.811750	-0.011663	1.744804
59.380806	887.192173	4.816755	-0.011759	1.751485
59.656450	895.367531	4.821760	-0.011816	1.758117
59.882112	903.539841	4.826765	-0.011864	1.764714
60.385563	911.675889	4.831770	-0.011963	1.771293
60.650538	919.845328	4.836774	-0.012018	1.777844
60.736704	928.039147	4.841779	-0.012040	1.784369
61.204182	936.179803	4.846784	-0.012132	1.790874
61.787458	944.327444	4.851789	-0.012246	1.797375
61.978992	952.480310	4.856794	-0.012287	1.803809
62.147323	960.623179	4.861798	-0.012324	1.810210
62.783758	968.734794	4.866803	-0.012448	1.816620
63.154416	976.852162	4.871808	-0.012523	1.822980
63.635227	984.991577	4.876813	-0.012618	1.829347
64.004496	993.139348	4.881818	-0.012692	1.835686
64.232198	1001.282365	4.886822	-0.012740	1.841983
64.736430	1009.408817	4.891827	-0.012839	1.848277
65.039174	1017.560399	4.896832	-0.012901	1.854546
65.396147	1025.697512	4.901837	-0.012973	1.860789
65.471541	1033.869936	4.906842	-0.012993	1.867005
65.920086	1042.013563	4.911846	-0.013082	1.873222
66.313744	1050.131703	4.916851	-0.013161	1.879392
66.512084	1058.246972	4.921856	-0.013203	1.885518
66.728249	1066.402397	4.926861	-0.013249	1.891656
67.320372	1074.481401	4.931866	-0.013365	1.897759
67.718329	1082.583662	4.936870	-0.013444	1.903839
68.091752	1090.727077	4.941875	-0.013519	1.909926
68.380366	1098.847541	4.946880	-0.013579	1.915967
68.947551	1106.940599	4.951885	-0.013690	1.922001
69.301511	1115.057333	4.956890	-0.013761	1.928009
69.630596	1123.205599	4.961894	-0.013828	1.934018
69.906681	1131.346418	4.966899	-0.013885	1.939998
69.875820	1139.506168	4.971904	-0.013884	1.945939
70.315801	1147.654632	4.976909	-0.013972	1.951905
70.707140	1155.750651	4.981914	-0.014050	1.957810
70.960078	1163.835663	4.986918	-0.014103	1.963674
71.369766	1171.950970	4.991923	-0.014185	1.969559
71.600963	1180.061142	4.996928	-0.014233	1.975404
72.026409	1188.148453	5.001933	-0.014318	1.981236
72.314390	1196.255238	5.006938	-0.014377	1.987050
72.383781	1204.411719	5.011942	-0.014395	1.992859
72.871866	1212.486478	5.016947	-0.014492	1.998637
73.098448	1220.569873	5.021952	-0.014539	2.004377
73.371989	1228.694744	5.026957	-0.014596	2.010135
73.732098	1236.798337	5.031962	-0.014668	2.015870
74.068313	1244.878241	5.036966	-0.014737	2.021570
74.516611	1252.982149	5.041971	-0.014825	2.027282
74.664382	1261.132719	5.046976	-0.014859	2.032979
74.991187	1269.223292	5.051981	-0.014925	2.038638
75.494581	1277.276407	5.056986	-0.015024	2.044272
75.685072	1285.384962	5.061990	-0.015065	2.049897
76.078480	1293.501419	5.066995	-0.015144	2.055533
76.412562	1301.582556	5.072000	-0.015211	2.061123
76.853349	1309.660064	5.077005	-0.015299	2.066706
76.872995	1317.831762	5.082010	-0.015308	2.072297
77.159022	1325.912936	5.087014	-0.015367	2.077837
77.496003	1334.000231	5.092019	-0.015435	2.083371
77.790542	1342.082073	5.097024	-0.015495	2.088883
78.036164	1350.206471	5.102029	-0.015547	2.094404
78.517832	1358.263865	5.107034	-0.015642	2.099888
78.582238	1366.377576	5.112038	-0.015659	2.105356
78.886494	1374.514559	5.117043	-0.015721	2.110847
79.260177	1382.609737	5.122048	-0.015797	2.116304
79.609660	1390.665706	5.127053	-0.015867	2.121717
79.678278	1398.777342	5.132058	-0.015885	2.127127
80.032049	1406.850585	5.137062	-0.015957	2.132525
80.345154	1414.934842	5.142067	-0.016020	2.137913
80.693514	1422.984095	5.147072	-0.016091	2.143267
80.743273	1431.117135	5.152077	-0.016106	2.148635
81.143713	1439.200698	5.157082	-0.016186	2.153990
81.394770	1447.269095	5.162086	-0.016238	2.159307
81.822470	1455.333826	5.167091	-0.016323	2.164626
82.279658	1463.390350	5.172096	-0.016413	2.169929
82.486051	1471.514123	5.177101	-0.016457	2.175239
82.663732	1479.607148	5.182106	-0.016496	2.180514
82.922854	1487.684494	5.187110	-0.016550	2.185773
83.441128	1495.782746	5.192115	-0.016652	2.191056
83.694694	1503.877322	5.197120	-0.016704	2.196301
83.886196	1511.953337	5.202125	-0.016746	2.201515
84.524696	1519.981957	5.207130	-0.016870	2.206727
84.872243	1528.057594	5.212134	-0.016940	2.211930
85.342662	1536.145751	5.217139	-0.017033	2.217140
85.437054	1544.231076	5.222144	-0.017056	2.222302
85.696115	1552.308747	5.227149	-0.017110	2.227462
86.045355	1560.402081	5.232154	-0.017180	2.232628
86.536365	1568.442008	5.237158	-0.017277	2.237761
86.765840	1576.537041	5.242163	-0.017325	2.242894
87.101181	1584.602545	5.247168	-0.017393	2.248005
87.509435	1592.697386	5.252173	-0.017475	2.253130
87.826196	1600.775599	5.257178	-0.017539	2.258224
87.798685	1608.874405	5.262182	-0.017540	2.263290
88.303581	1616.940290	5.267187	-0.017639	2.268370
88.674912	1625.073226	5.272192	-0.017714	2.273469
88.914732	1633.133772	5.277197	-0.017764	2.278500
89.461175	1641.157372	5.282202	-0.017871	2.283524
89.482404	1649.247473	5.287206	-0.017881	2.288532
89.874178	1657.336946	5.292211	-0.017959	2.293561
89.995104	1665.400794	5.297216	-0.017987	2.298539
90.375737	1673.454951	5.302221	-0.018063	2.303523
90.606753	1681.530784	5.307226	-0.018112	2.308497
90.946705	1689.601887	5.312230	-0.018181	2.313467
91.396178	1697.647220	5.317235	-0.018270	2.318418
91.553135	1705.710787	5.322240	-0.018304	2.323347
91.782937	1713.790912	5.327245	-0.018353	2.328280
91.872451	1721.907444	5.332250	-0.018375	2.333214
92.310895	1729.930067	5.337254	-0.018462	2.338109
92.785715	1737.977284	5.342259	-0.018556	2.343012
93.119298	1746.039849	5.347264	-0.018623	2.347902
93.267929	1754.173055	5.352269	-0.018656	2.352809
93.510588	1762.238315	5.357274	-0.018707	2.357673
93.892816	1770.261419	5.362278	-0.018784	2.362512
94.041738	1778.348882	5.367283	-0.018817	2.367362
94.536512	1786.391052	5.372288	-0.018915	2.372202
94.569328	1794.495802	5.377293	-0.018926	2.377033
94.951335	1802.538938	5.382298	-0.019003	2.381844
95.295236	1810.589751	5.387302	-0.019072	2.386648
95.739813	1818.673378	5.392307	-0.019160	2.391469
95.936671	1826.734786	5.397312	-0.019203	2.396248
96.011614	1834.817032	5.402317	-0.019222	2.401020
96.338526	1842.867785	5.407322	-0.019288	2.405784
96.734589	1850.914349	5.412326	-0.019368	2.410541
96.981329	1859.015037	5.417331	-0.019419	2.415309
97.179048	1867.060416	5.422336	-0.019461	2.420031
97.434423	1875.123114	5.427341	-0.019514	2.424759
97.691436	1883.207674	5.432346	-0.019568	2.429490
97.972002	1891.337034	5.437350	-0.019625	2.434239
98.397901	1899.349442	5.442355	-0.019710	2.438923
98.547015	1907.380259	5.447360	-0.019743	2.443587
98.926266	1915.404113	5.452365	-0.019819	2.448256
98.919932	1923.524738	5.457370	-0.019824	2.452942
98.886795	1931.584393	5.462374	-0.019823	2.457582
99.198994	1939.644791	5.467379	-0.019887	2.462240
99.760025	1947.638050	5.472384	-0.019996	2.466869
100.249755	1955.697459	5.477389	-0.020093	2.471522
100.507103	1963.783793	5.482394	-0.020146	2.476164
100.374589	1971.863898	5.487398	-0.020127	2.480765
100.734142	1979.909287	5.492403	-0.020200	2.485374
101.013357	1987.951409	5.497408	-0.020257	2.489967
101.049905	1996.041640	5.502413	-0.020269	2.494560
101.315132	2004.092424	5.507418	-0.020324	2.499140
101.622677	2012.124224	5.512422	-0.020387	2.503703
101.828809	2020.206380	5.517427	-0.020431	2.508279
102.184050	2028.286186	5.522432	-0.020502	2.512857
102.533955	2036.311061	5.527437	-0.020573	2.517394
102.776681	2044.370243	5.532442	-0.020624	2.521935
102.836112	2052.408471	5.537446	-0.020640	2.526443
103.150339	2060.490531	5.542451	-0.020704	2.530985
103.360375	2068.549965	5.547456	-0.020749	2.535499
103.582383	2076.583402	5.552461	-0.020795	2.539991
103.771538	2084.639324	5.557466	-0.020836	2.544486
104.077227	2092.675667	5.562470	-0.020899	2.548970
104.203619	2100.800421	5.567475	-0.020928	2.553482
104.497961	2108.814999	5.572480	-0.020988	2.557938
105.347049	2116.793334	5.577485	-0.021151	2.562404
105.593525	2124.864532	5.582490	-0.021203	2.566871
105.801611	2132.942306	5.587494	-0.021247	2.571332
106.151030	2141.014450	5.592499	-0.021317	2.575791
106.101539	2149.087173	5.597504	-0.021314	2.580216
106.242188	2157.135588	5.602509	-0.021345	2.584632
106.343377	2165.219105	5.607514	-0.021370	2.589058
106.712151	2173.412727	5.612518	-0.021444	2.593554
107.094763	2181.443832	5.617523	-0.021521	2.597955
106.793141	2189.467312	5.622528	-0.021470	2.602298
107.131216	2197.460864	5.627533	-0.021538	2.606661
107.291870	2205.505081	5.632538	-0.021574	2.611032
107.571130	2213.536024	5.637542	-0.021631	2.615396
107.802217	2221.587688	5.642547	-0.021679	2.619761
108.156508	2229.589293	5.647552	-0.021751	2.624100
108.394710	2237.659048	5.652557	-0.021801	2.628460
108.566326	2245.718601	5.657562	-0.021838	2.632803
108.747633	2253.763885	5.662566	-0.021877	2.637133
109.050761	2261.801977	5.667571	-0.021939	2.641459
109.094413	2269.849966	5.672576	-0.021953	2.645766
109.660286	2277.853783	5.677581	-0.022064	2.650077
110.065190	2285.904462	5.682586	-0.022144	2.654395
110.122400	2293.963161	5.687590	-0.022161	2.658688
110.556041	2301.999563	5.692595	-0.022247	2.662986
111.117129	2310.016013	5.697600	-0.022357	2.667275
111.227648	2318.113506	5.702605	-0.022383	2.671571
111.388272	2326.199702	5.707610	-0.022418	2.675857
111.574434	2334.216564	5.712614	-0.022458	2.680102
111.837912	2342.235704	5.717619	-0.022513	2.684345
112.000766	2350.283423	5.722624	-0.022548	2.688591
112.323260	2358.353837	5.727629	-0.022614	2.692852
112.755529	2366.393031	5.732634	-0.022700	2.697097
112.717615	2374.462344	5.737638	-0.022698	2.701321
113.048391	2382.483261	5.742643	-0.022765	2.705536
113.232764	2390.535641	5.747648	-0.022805	2.709752
113.244286	2398.631559	5.752653	-0.022813	2.713973
113.527967	2406.664348	5.757658	-0.022871	2.718172
113.749348	2414.663656	5.762662	-0.022918	2.722343
114.098075	2422.724022	5.767667	-0.022988	2.726547
114.285803	2430.768546	5.772672	-0.023028	2.730726
114.591426	2438.819966	5.777677	-0.023091	2.734910
114.931340	2446.871971	5.782682	-0.023160	2.739090
114.998696	2454.906335	5.787686	-0.023178	2.743238
115.304187	2462.946610	5.792691	-0.023240	2.747396
115.586815	2471.014710	5.797696	-0.023298	2.751562
115.862404	2479.121596	5.802701	-0.023355	2.755740
115.943061	2487.143185	5.807706	-0.023375	2.759857
116.120901	2495.138538	5.812710	-0.023414	2.763960
116.539409	2503.164750	5.817715	-0.023497	2.768087
116.642198	2511.232775	5.822720	-0.023522	2.772210
116.859050	2519.276256	5.827725	-0.023568	2.776321
117.115731	2527.313637	5.832730	-0.023621	2.780426
117.222176	2535.332566	5.837734	-0.023646	2.784506
117.459514	2543.402312	5.842739	-0.023696	2.788614
117.825604	2551.430920	5.847744	-0.023769	2.792702
117.968950	2559.498540	5.852749	-0.023801	2.796791
118.141114	2567.547504	5.857754	-0.023839	2.800866
118.464735	2575.520186	5.862758	-0.023905	2.804906
118.936498	2583.566893	5.867763	-0.023998	2.808985
118.991565	2591.654245	5.872768	-0.024014	2.813055
119.284320	2599.676895	5.877773	-0.024074	2.817100
119.728260	2607.723824	5.882778	-0.024162	2.821160
119.841859	2615.757383	5.887782	-0.024188	2.825189
120.239929	2623.803098	5.892787	-0.024268	2.829234
120.284236	2631.903411	5.897792	-0.024282	2.833280
120.760148	2639.909788	5.902797	-0.024376	2.837299
120.739679	2647.969148	5.907802	-0.024377	2.841310
121.063016	2655.963169	5.912806	-0.024443	2.845302
121.445292	2663.996541	5.917811	-0.024520	2.849311
121.664214	2672.058660	5.922816	-0.024566	2.853320
121.629676	2680.121728	5.927821	-0.024565	2.857309
121.941251	2688.160207	5.932826	-0.024628	2.861300
122.017596	2696.178956	5.937830	-0.024648	2.865262
122.575160	2704.191571	5.942835	-0.024757	2.869243
122.608895	2712.276892	5.947840	-0.024769	2.873225
122.927217	2720.311734	5.952845	-0.024834	2.877192
123.152764	2728.340845	5.957850	-0.024881	2.881145
123.256131	2736.363513	5.962854	-0.024906	2.885084
123.607539	2744.425117	5.967859	-0.024977	2.889049
123.926867	2752.456825	5.972864	-0.025042	2.892993
124.309783	2760.494540	5.977869	-0.025118	2.896938
124.541398	2768.560183	5.982874	-0.025167	2.900882
124.505122	2776.577356	5.987878	-0.025166	2.904784
124.731623	2784.640552	5.992883	-0.025213	2.908716
124.872702	2792.746079	5.997888	-0.025245	2.912659
125.212764	2800.796980	6.002893	-0.025314	2.916581
125.424450	2808.807837	6.007898	-0.025359	2.920471
125.699892	2816.773412	6.012902	-0.025415	2.924338
125.892334	2824.818277	6.017907	-0.025457	2.928233
126.015753	2832.871786	6.022912	-0.025485	2.932124
126.203462	2840.918032	6.027917	-0.025525	2.936009
126.428233	2848.944383	6.032922	-0.025573	2.939882
126.590194	2856.951847	6.037926	-0.025608	2.943737
126.833009	2864.991092	6.042931	-0.025659	2.947606
127.017399	2873.049969	6.047936	-0.025699	2.951477
127.435001	2881.080629	6.052941	-0.025782	2.955341
127.731561	2889.108929	6.057946	-0.025843	2.959193
127.788472	2897.114730	6.062950	-0.025859	2.963016
128.027655	2905.181464	6.067955	-0.025909	2.966873
128.282633	2913.215131	6.072960	-0.025962	2.970710
128.466604	2921.259042	6.077965	-0.026001	2.974543
128.770165	2929.311843	6.082970	-0.026063	2.978382
128.960827	2937.326624	6.087974	-0.026104	2.982192
129.166903	2945.368594	6.092979	-0.026148	2.986010
129.377395	2953.398705	6.097984	-0.026193	2.989818
129.584433	2961.483856	6.102989	-0.026237	2.993647
129.959973	2969.503356	6.107994	-0.026312	2.997449
130.119471	2977.522253	6.112998	-0.026347	3.001235
130.547658	2985.522361	6.118003	-0.026432	3.005020
131.005371	2993.548959	6.123008	-0.026523	3.008815
131.001390	3001.627800	6.128013	-0.026528	3.012606
131.043847	3009.706621	6.133018	-0.026541	3.016395
131.514663	3017.672036	6.138022	-0.026634	3.020147
131.864389	3025.723739	6.143027	-0.026705	3.023929
131.803200	3033.785089	6.148032	-0.026699	3.027690
132.087669	3041.821122	6.153037	-0.026757	3.031452
132.388427	3049.889072	6.158042	-0.026819	3.035224
132.343076	3057.882926	6.163046	-0.026816	3.038941
132.912410	3065.874680	6.168051	-0.026927	3.042682
133.226611	3073.900244	6.173056	-0.026991	3.046421
133.207494	3081.973587	6.178061	-0.026993	3.050163
133.465534	3090.034382	6.183066	-0.027046	3.053906
133.630351	3098.041818	6.188070	-0.027083	3.057617
133.989225	3106.081113	6.193075	-0.027155	3.061346
134.260285	3114.085885	6.198080	-0.027211	3.065051
134.326804	3122.142409	6.203085	-0.027229	3.068766
134.689810	3130.243683	6.208090	-0.027302	3.072510
134.521962	3138.340404	6.213094	-0.027276	3.076223
135.052950	3146.288725	6.218099	-0.027380	3.079896
135.304849	3154.258755	6.223104	-0.027432	3.083562
135.309457	3162.324146	6.228109	-0.027439	3.087255
135.780775	3170.362998	6.233114	-0.027532	3.090953
136.018567	3178.392867	6.238118	-0.027582	3.094632
136.031715	3186.443380	6.243123	-0.027590	3.098306
136.239970	3194.450283	6.248128	-0.027634	3.101964
136.444985	3202.462272	6.253133	-0.027677	3.105621
136.856079	3210.514736	6.258138	-0.027759	3.109300
136.932212	3218.567742	6.263142	-0.027779	3.112960
137.008628	3226.603382	6.268147	-0.027799	3.116608
137.175824	3234.627045	6.273152	-0.027835	3.120251
137.256953	3242.633508	6.278157	-0.027856	3.123877
137.569542	3250.678236	6.283162	-0.027919	3.127527
137.873178	3258.728569	6.288166	-0.027981	3.131175
138.028352	3266.777465	6.293171	-0.028016	3.134811
138.104851	3274.797067	6.298176	-0.028035	3.138427
138.231555	3282.817556	6.303181	-0.028064	3.142040
138.579258	3290.848618	6.308186	-0.028135	3.145664
138.744753	3298.875638	6.313190	-0.028171	3.149274
138.879697	3306.956056	6.318195	-0.028201	3.152903
139.349511	3314.994375	6.323200	-0.028294	3.156523
139.347972	3322.989548	6.328205	-0.028300	3.160099
139.349182	3331.029876	6.333210	-0.028305	3.163691
139.764006	3339.008469	6.338214	-0.028388	3.167269
140.204500	3347.055488	6.343219	-0.028475	3.170875
140.282011	3355.096412	6.348224	-0.028495	3.174459
140.348465	3363.160177	6.353229	-0.028513	3.178048
140.439312	3371.193484	6.358234	-0.028535	3.181620
140.670492	3379.188620	6.363238	-0.028584	3.185178
140.913082	3387.232600	6.368243	-0.028634	3.188753
141.271176	3395.262708	6.373248	-0.028707	3.192324
141.459370	3403.323842	6.378253	-0.028747	3.195896
141.461336	3411.346759	6.383258	-0.028753	3.199441
141.666581	3419.341578	6.388262	-0.028797	3.202977
141.886622	3427.394260	6.393267	-0.028843	3.206535
142.408765	3435.403311	6.398272	-0.028946	3.210083
142.398623	3443.472431	6.403277	-0.028949	3.213631
142.746064	3451.496174	6.408282	-0.029019	3.217170
142.858933	3459.491179	6.413286	-0.029046	3.220683
142.898513	3467.531068	6.418291	-0.029059	3.224209
143.352344	3475.562417	6.423296	-0.029149	3.227744
143.651820	3483.622219	6.428301	-0.029210	3.231281
143.939806	3491.716389	6.433306	-0.029269	3.234829
144.050405	3499.671457	6.438310	-0.029295	3.238305
144.646878	3507.678895	6.443315	-0.029411	3.241820
144.771591	3515.695974	6.448320	-0.029440	3.245316
144.657912	3523.735181	6.453325	-0.029424	3.248808
145.618892	3531.736359	6.458330	-0.029609	3.252323
145.846802	3539.793986	6.463334	-0.029657	3.255829
146.205149	3547.811694	6.468339	-0.029729	3.259320
146.563494	3555.837459	6.473344	-0.029801	3.262810
146.806946	3563.863011	6.478349	-0.029852	3.266292
147.006574	3571.894746	6.483354	-0.029894	3.269770
147.015317	3579.961203	6.488358	-0.029901	3.273253
147.374700	3587.993538	6.493363	-0.029974	3.276731
147.685821	3596.004884	6.498368	-0.030037	3.280194
147.624803	3604.036020	6.503373	-0.030031	3.283648
147.945291	3612.073121	6.508378	-0.030096	3.287115
148.121106	3620.078073	6.513382	-0.030134	3.290559
148.194121	3628.164827	6.518387	-0.030153	3.294031
148.380837	3636.187995	6.523392	-0.030194	3.297476
148.928081	3644.192493	6.528397	-0.030301	3.300923
149.249209	3652.203909	6.533402	-0.030366	3.304361
149.291305	3660.220904	6.538406	-0.030380	3.307787
149.754835	3668.265869	6.543411	-0.030471	3.311238
149.766997	3676.347042	6.548416	-0.030479	3.314683
150.038573	3684.324177	6.553421	-0.030535	3.318090
150.090011	3692.385636	6.558426	-0.030550	3.321521
150.283396	3700.374589	6.563430	-0.030591	3.324923
150.548688	3708.399351	6.568435	-0.030646	3.328340
150.660149	3716.456302	6.573440	-0.030672	3.331760
150.760661	3724.501170	6.578445	-0.030697	3.335172
150.985365	3732.531673	6.583450	-0.030744	3.338579
151.162641	3740.531033	6.588454	-0.030782	3.341967
151.559639	3748.538726	6.593459	-0.030862	3.345364
151.537763	3756.580734	6.598464	-0.030863	3.348756
151.516934	3764.645626	6.603469	-0.030865	3.352154
151.852604	3772.701259	6.608474	-0.030933	3.355558
151.878682	3780.695378	6.613478	-0.030943	3.358921
152.324496	3788.708269	6.618483	-0.031031	3.362304
152.321148	3796.756080	6.623488	-0.031036	3.365682
152.547195	3804.728285	6.628493	-0.031084	3.369033
152.872490	3812.821605	6.633498	-0.031150	3.372435
152.944769	3820.860477	6.638502	-0.031169	3.375802
153.214142	3828.849567	6.643507	-0.031224	3.379152
153.385981	3836.871446	6.648512	-0.031262	3.382508
153.500370	3844.900254	6.653517	-0.031288	3.385862
153.749458	3852.947444	6.658522	-0.031340	3.389225
153.909939	3861.022218	6.663526	-0.031376	3.392593
153.829244	3869.106597	6.668531	-0.031366	3.395953
154.036269	3877.056825	6.673536	-0.031410	3.399265
154.138362	3885.035724	6.678541	-0.031434	3.402581
154.571453	3893.046047	6.683546	-0.031520	3.405918
154.623667	3901.061477	6.688550	-0.031536	3.409241
154.825365	3909.126670	6.693555	-0.031579	3.412587
155.084047	3917.172499	6.698560	-0.031632	3.415923
155.399989	3925.142202	6.703565	-0.031696	3.419226
155.622890	3933.186472	6.708570	-0.031743	3.422554
155.964660	3941.194813	6.713574	-0.031812	3.425868
156.107360	3949.237276	6.718579	-0.031844	3.429186
156.260046	3957.301206	6.723584	-0.031878	3.432509
156.459338	3965.335034	6.728589	-0.031921	3.435819
156.887246	3973.317770	6.733594	-0.032006	3.439112
156.970821	3981.314288	6.738598	-0.032027	3.442396
157.356269	3989.343527	6.743603	-0.032104	3.445700
157.421653	3997.383682	6.748608	-0.032122	3.448995
157.386245	4005.451916	6.753613	-0.032121	3.452295
157.531948	4013.504869	6.758618	-0.032153	3.455592
158.039573	4021.481438	6.763622	-0.032253	3.458866
157.909880	4029.519185	6.768627	-0.032235	3.462141
158.178171	4037.544165	6.773632	-0.032290	3.465420
158.383688	4045.581119	6.778637	-0.032334	3.468700
158.730797	4053.632176	6.783642	-0.032404	3.471986
158.835557	4061.657237	6.788646	-0.032429	3.475251
159.088206	4069.656653	6.793651	-0.032481	3.478508
159.225487	4077.694360	6.798656	-0.032512	3.481773
159.170896	4085.670793	6.803661	-0.032507	3.485004
159.408009	4093.741226	6.808666	-0.032557	3.488279
159.647604	4101.735004	6.813670	-0.032607	3.491520
159.913359	4109.765970	6.818675	-0.032662	3.494774
160.244692	4117.807172	6.823680	-0.032729	3.498031
160.524684	4125.778721	6.828685	-0.032787	3.501256
160.852501	4133.813721	6.833690	-0.032853	3.504504
160.828467	4141.873490	6.838694	-0.032854	3.507749
161.035157	4149.897277	6.843699	-0.032898	3.510983
161.292747	4157.937078	6.848704	-0.032951	3.514222
161.266783	4165.945533	6.853709	-0.032952	3.517436
161.480060	4173.981127	6.858714	-0.032997	3.520667
161.636600	4181.965416	6.863718	-0.033032	3.523871
161.915831	4190.004641	6.868723	-0.033089	3.527099
162.083823	4198.062950	6.873728	-0.033126	3.530328
162.351736	4206.083629	6.878733	-0.033181	3.533541
162.604943	4214.144142	6.883738	-0.033234	3.536768
162.677269	4222.143582	6.888742	-0.033253	3.539961
162.725356	4230.159163	6.893747	-0.033267	3.543157
162.919882	4238.203960	6.898752	-0.033309	3.546367
162.924228	4246.224064	6.903757	-0.033315	3.549558
163.183289	4254.337663	6.908762	-0.033369	3.552791
163.341237	4262.383730	6.913766	-0.033404	3.555991
163.577625	4270.328172	6.918771	-0.033453	3.559150
163.663415	4278.342950	6.923776	-0.033474	3.562330
163.997596	4286.315031	6.928781	-0.033542	3.565497
164.287975	4294.350473	6.933786	-0.033602	3.568685
164.359533	4302.370618	6.938790	-0.033620	3.571858
164.377900	4310.438210	6.943795	-0.033629	3.575045
164.697177	4318.439565	6.948800	-0.033694	3.578212
164.835981	4326.446274	6.953805	-0.033725	3.581373
164.882821	4334.451755	6.958810	-0.033740	3.584528
165.070548	4342.500121	6.963814	-0.033780	3.587702
165.404950	4350.540326	6.968819	-0.033848	3.590873
165.621038	4358.577258	6.973824	-0.033893	3.594037
165.762739	4366.564669	6.978829	-0.033925	3.597176
166.023707	4374.556143	6.983834	-0.033979	3.600318
166.175867	4382.556931	6.988838	-0.034013	3.603457
166.194847	4390.621349	6.993843	-0.034022	3.606615
166.477372	4398.636560	6.998848	-0.034080	3.609758
166.696773	4406.662576	7.003853	-0.034126	3.612901
166.841938	4414.734537	7.008858	-0.034159	3.616057
166.885717	4422.715908	7.013862	-0.034172	3.619173
167.390100	4430.731844	7.018867	-0.034272	3.622311
167.481341	4438.764731	7.023872	-0.034294	3.625442
167.572722	4446.787744	7.028877	-0.034316	3.628567
167.963895	4454.857843	7.033882	-0.034395	3.631715
167.939866	4462.935094	7.038886	-0.034396	3.634852
168.036901	4470.925610	7.043891	-0.034419	3.637956
168.481550	4478.923094	7.048896	-0.034507	3.641069
168.537573	4486.902066	7.053901	-0.034523	3.644162
168.847663	4494.953457	7.058906	-0.034587	3.647287
169.046301	4502.953337	7.063910	-0.034629	3.650387
169.245961	4511.013384	7.068915	-0.034672	3.653507
169.297463	4519.052515	7.073920	-0.034687	3.656612
169.259079	4527.043100	7.078925	-0.034685	3.659694
169.687629	4535.067055	7.083930	-0.034770	3.662798
169.959431	4543.095650	7.088934	-0.034826	3.665897
170.121580	4551.105291	7.093939	-0.034862	3.668984
170.518642	4559.166062	7.098944	-0.034941	3.672093
170.691243	4567.161103	7.103949	-0.034979	3.675169
170.971339	4575.207813	7.108954	-0.035036	3.678265
170.985966	4583.221321	7.113958	-0.035044	3.681339
171.307150	4591.194250	7.118963	-0.035110	3.684402
171.509545	4599.269948	7.123968	-0.035153	3.687499
171.507351	4607.283598	7.128973	-0.035158	3.690564
172.015570	4615.303768	7.133978	-0.035258	3.693643
172.192466	4623.325654	7.138982	-0.035296	3.696711
172.189284	4631.325985	7.143987	-0.035301	3.699763
172.544563	4639.352103	7.148992	-0.035373	3.702832
172.696981	4647.380225	7.153997	-0.035407	3.705894
172.972778	4655.427562	7.159002	-0.035463	3.708964
172.853520	4663.503996	7.164006	-0.035447	3.712033
173.107239	4671.553122	7.169011	-0.035499	3.715098
173.255104	4679.519584	7.174016	-0.035532	3.718126
173.204515	4687.531694	7.179021	-0.035528	3.721164
173.698991	4695.477560	7.184026	-0.035626	3.724188
173.671016	4703.544251	7.189030	-0.035626	3.727243
173.771019	4711.547517	7.194035	-0.035650	3.730274
173.887406	4719.619081	7.199040	-0.035677	3.733329
174.017033	4727.605545	7.204045	-0.035707	3.736349
174.328202	4735.606953	7.209050	-0.035770	3.739377
174.584572	4743.635821	7.214054	-0.035823	3.742412
174.747391	4751.701218	7.219059	-0.035859	3.745456
174.956109	4759.718139	7.224064	-0.035903	3.748480
174.910166	4767.727599	7.229069	-0.035900	3.751492
175.074949	4775.789393	7.234074	-0.035936	3.754527
175.399258	4783.778920	7.239078	-0.036002	3.757536
175.559441	4791.804255	7.244083	-0.036037	3.760552
175.771238	4799.817118	7.249088	-0.036082	3.763563
175.770407	4807.834521	7.254093	-0.036088	3.766567
176.048670	4815.847129	7.259098	-0.036145	3.769574
175.852189	4823.913526	7.264102	-0.036114	3.772588
176.265990	4831.910836	7.269107	-0.036196	3.775587
176.386481	4839.977581	7.274112	-0.036224	3.778603
176.794455	4847.993338	7.279117	-0.036305	3.781604
176.992417	4855.995609	7.284122	-0.036348	3.784593
177.162362	4864.016036	7.289126	-0.036385	3.787586
177.425772	4872.017178	7.294131	-0.036439	3.790571
177.465365	4880.109419	7.299136	-0.036452	3.793583
177.754000	4888.104295	7.304141	-0.036511	3.796562
178.127871	4896.113997	7.309146	-0.036586	3.799546
178.102167	4904.108273	7.314150	-0.036587	3.802512
178.297675	4912.104218	7.319155	-0.036629	3.805482
178.486368	4920.131340	7.324160	-0.036669	3.808461
178.620964	4928.184017	7.329165	-0.036700	3.811446
178.675455	4936.203840	7.334170	-0.036715	3.814415
179.023824	4944.220515	7.339174	-0.036786	3.817387
179.225192	4952.226723	7.344179	-0.036829	3.820349
179.349876	4960.263113	7.349184	-0.036857	3.823318
179.442354	4968.238229	7.354189	-0.036880	3.826262
179.795044	4976.274142	7.359194	-0.036951	3.829231
179.969198	4984.330866	7.364198	-0.036989	3.832202
179.975949	4992.360147	7.369203	-0.036996	3.835157
180.262003	5000.366237	7.374208	-0.037054	3.838107
180.400751	5008.366525	7.379213	-0.037086	3.841050
180.536287	5016.382553	7.384218	-0.037116	3.843995
180.684074	5024.393894	7.389222	-0.037149	3.846938
180.794255	5032.427171	7.394227	-0.037175	3.849885
181.198439	5040.496349	7.399232	-0.037256	3.852849
181.238904	5048.504193	7.404237	-0.037269	3.855781
181.763933	5056.519577	7.409242	-0.037372	3.858723
181.553398	5064.555297	7.414246	-0.037338	3.861655
181.751998	5072.543819	7.419251	-0.037381	3.864577
182.018265	5080.600685	7.424256	-0.037436	3.867522
182.124218	5088.592028	7.429261	-0.037461	3.870438
182.515383	5096.851717	7.434266	-0.037539	3.873455
182.628509	5104.859386	7.439270	-0.037566	3.876373
182.697449	5112.740736	7.444275	-0.037584	3.879241
182.930447	5120.778096	7.449280	-0.037633	3.882167
183.018812	5128.719306	7.454285	-0.037655	3.885054
183.082609	5136.715100	7.459290	-0.037672	3.887957
183.179282	5144.764244	7.464294	-0.037695	3.890878
183.296964	5152.802863	7.469299	-0.037723	3.893794
183.732990	5160.801470	7.474304	-0.037809	3.896699
183.844859	5168.790461	7.479309	-0.037836	3.899592
184.051355	5176.846997	7.484314	-0.037880	3.902509
184.215156	5184.856563	7.489318	-0.037915	3.905407
184.477634	5192.873088	7.494323	-0.037970	3.908306
184.638960	5200.934676	7.499328	-0.038005	3.911218
185.039573	5208.927647	7.504333	-0.038085	3.914107
185.322689	5216.942270	7.509338	-0.038143	3.916999
185.306137	5224.922743	7.514342	-0.038146	3.919872
185.427897	5232.937622	7.519347	-0.038174	3.922757
185.773525	5240.966217	7.524352	-0.038244	3.925649
186.061709	5248.955099	7.529357	-0.038303	3.928524
186.349560	5257.031774	7.534362	-0.038362	3.931428
186.481409	5265.071871	7.539366	-0.038392	3.934314
186.643440	5273.089413	7.544371	-0.038427	3.937190
186.914084	5281.074349	7.549376	-0.038483	3.940055
187.009382	5289.086129	7.554381	-0.038506	3.942924
187.300276	5297.097627	7.559386	-0.038566	3.945794
187.298088	5305.128631	7.564390	-0.038571	3.948663
187.430949	5313.178985	7.569395	-0.038601	3.951540
187.645086	5321.226928	7.574400	-0.038646	3.954416
187.840871	5329.241427	7.579405	-0.038688	3.957277
188.023088	5337.206373	7.584410	-0.038728	3.960118
188.098103	5345.241941	7.589414	-0.038747	3.962980
188.328692	5353.218828	7.594419	-0.038795	3.965822
188.597599	5361.255053	7.599424	-0.038851	3.968684
188.505090	5369.271339	7.604429	-0.038839	3.971530
188.824912	5377.352961	7.609434	-0.038904	3.974404
189.155009	5385.331805	7.614438	-0.038971	3.977240
188.993895	5393.345768	7.619443	-0.038947	3.980079
189.470998	5401.348714	7.624448	-0.039041	3.982921
189.680088	5409.390384	7.629453	-0.039085	3.985772
189.599429	5417.434594	7.634458	-0.039076	3.988616
189.788894	5425.502945	7.639462	-0.039116	3.991471
190.072244	5433.499448	7.644467	-0.039175	3.994300
190.164004	5441.545046	7.649472	-0.039197	3.997141
190.314775	5449.512257	7.654477	-0.039231	3.999954
190.633680	5457.541297	7.659482	-0.039295	4.002789
190.628876	5465.544724	7.664486	-0.039300	4.005608
190.692314	5473.538295	7.669491	-0.039317	4.008422
191.157723	5481.634015	7.674496	-0.039409	4.011277
191.390371	5489.625264	7.679501	-0.039458	4.014089
191.650876	5497.677893	7.684506	-0.039512	4.016922
191.685535	5505.675143	7.689510	-0.039524	4.019729
191.949223	5513.664338	7.694515	-0.039578	4.022535
191.981078	5521.706841	7.699520	-0.039590	4.025354
192.163545	5529.716313	7.704525	-0.039629	4.028162
192.504451	5537.746870	7.709530	-0.039698	4.030978
192.640783	5545.872430	7.714534	-0.039729	4.033822
192.721955	5553.866763	7.719539	-0.039749	4.036617
192.922861	5561.798938	7.724544	-0.039792	4.039390
192.994188	5569.806627	7.729549	-0.039811	4.042186
193.085146	5577.834285	7.734554	-0.039833	4.044987
193.148933	5585.855263	7.739558	-0.039851	4.047783
193.483245	5593.865031	7.744563	-0.039918	4.050578
193.648116	5601.909129	7.749568	-0.039954	4.053380
193.751655	5609.912942	7.754573	-0.039979	4.056165
194.028634	5617.884539	7.759578	-0.040036	4.058939
194.231882	5625.948395	7.764582	-0.040079	4.061743
194.235594	5633.925354	7.769587	-0.040086	4.064512
194.342963	5641.987253	7.774592	-0.040111	4.067309
194.669058	5649.971938	7.779597	-0.040177	4.070081
194.952383	5658.001820	7.784602	-0.040235	4.072866
194.911810	5666.067563	7.789606	-0.040233	4.075657
195.218895	5674.015581	7.794611	-0.040296	4.078411
195.526552	5682.065765	7.799616	-0.040359	4.081197
195.554448	5690.030559	7.804621	-0.040369	4.083949
195.823262	5698.126913	7.809626	-0.040425	4.086747
195.900108	5706.107033	7.814630	-0.040444	4.089501
196.010812	5714.125672	7.819635	-0.040470	4.092266
196.098446	5722.178796	7.824640	-0.040492	4.095041
196.386828	5730.193334	7.829645	-0.040551	4.097804
196.696603	5738.169909	7.834650	-0.040614	4.100552
196.724591	5746.190978	7.839654	-0.040625	4.103310
197.025469	5754.220652	7.844659	-0.040687	4.106072
197.253067	5762.285039	7.849664	-0.040734	4.108843
197.056277	5770.297317	7.854669	-0.040703	4.111590
197.269374	5778.346795	7.859674	-0.040748	4.114352
197.492364	5786.376795	7.864678	-0.040795	4.117106
197.597125	5794.315429	7.869683	-0.040820	4.119825
197.725901	5802.357963	7.874688	-0.040850	4.122578
197.920562	5810.330428	7.879693	-0.040891	4.125307
198.218394	5818.358398	7.884698	-0.040952	4.128053
198.273898	5826.410760	7.889702	-0.040968	4.130804
198.413224	5834.448084	7.894707	-0.040999	4.133548
198.610630	5842.500621	7.899712	-0.041042	4.136296
198.680742	5850.447703	7.904717	-0.041060	4.139005
199.052176	5858.524983	7.909722	-0.041135	4.141760
199.303175	5866.523987	7.914726	-0.041187	4.144485
199.207508	5874.540625	7.919731	-0.041174	4.147211
199.517057	5882.555606	7.924736	-0.041237	4.149938
199.621146	5890.604330	7.929741	-0.041262	4.152673
199.717518	5898.642117	7.934746	-0.041286	4.155402
199.919332	5906.629107	7.939750	-0.041329	4.158114
199.787430	5914.646698	7.944755	-0.041310	4.160830
200.173853	5922.629630	7.949760	-0.041387	4.163539
200.480913	5930.651992	7.954765	-0.041449	4.166258
200.555741	5938.670040	7.959770	-0.041469	4.168971
200.826242	5946.770838	7.964774	-0.041525	4.171713
200.861854	5954.712998	7.969779	-0.041537	4.174397
201.029068	5962.757667	7.974784	-0.041573	4.177115
201.321429	5970.743356	7.979789	-0.041633	4.179812
201.619838	5978.774885	7.984794	-0.041694	4.182524
201.606747	5986.821924	7.989798	-0.041697	4.185235
201.791352	5994.830673	7.994803	-0.041737	4.187934
202.000679	6002.856868	7.999808	-0.041781	4.190638
202.110491	6010.969532	8.004813	-0.041807	4.193367
202.155774	6018.985518	8.009818	-0.041821	4.196062
202.320737	6026.909913	8.014822	-0.041857	4.198725
202.686954	6034.901931	8.019827	-0.041931	4.201412
202.847808	6042.862818	8.024832	-0.041966	4.204084
203.037137	6050.876402	8.029837	-0.042007	4.206772
203.137070	6058.907280	8.034842	-0.042031	4.209464
203.296344	6066.967644	8.039846	-0.042066	4.212164
203.498104	6074.962886	8.044851	-0.042109	4.214841
203.580476	6083.003345	8.049856	-0.042130	4.217530
203.749628	6090.995896	8.054861	-0.042167	4.220203
203.922653	6098.989734	8.059866	-0.042204	4.222874
204.050738	6107.016249	8.064870	-0.042234	4.225554
204.249194	6115.042097	8.069875	-0.042276	4.228233
204.487052	6123.075716	8.074880	-0.042326	4.230912
204.676452	6131.106569	8.079885	-0.042367	4.233589
204.954387	6139.119388	8.084890	-0.042424	4.236259
204.907246	6147.127012	8.089894	-0.042420	4.238923
205.274163	6155.128780	8.094899	-0.042494	4.241586
205.380130	6163.127154	8.099904	-0.042519	4.244245
205.317778	6171.154145	8.104909	-0.042513	4.246909
205.620987	6179.154290	8.109914	-0.042575	4.249567
205.832002	6187.199804	8.114918	-0.042620	4.252237
206.135494	6195.246035	8.119923	-0.042682	4.254906
206.150364	6203.283664	8.124928	-0.042690	4.257568
206.072706	6211.259975	8.129933	-0.042681	4.260207
206.165161	6219.286656	8.134938	-0.042703	4.262863
206.577722	6227.316423	8.139942	-0.042786	4.265521
206.563141	6235.347613	8.144947	-0.042788	4.268175
206.666200	6243.375965	8.149952	-0.042813	4.270826
206.879146	6251.431085	8.154957	-0.042858	4.273486
207.157285	6259.482992	8.159962	-0.042915	4.276143
207.249389	6267.437744	8.164966	-0.042938	4.278765
207.373975	6275.461070	8.169971	-0.042967	4.281409
207.478983	6283.456701	8.174976	-0.042992	4.284041
207.543907	6291.504835	8.179981	-0.043009	4.286689
207.881033	6299.455208	8.184986	-0.043077	4.289305
207.889239	6307.532828	8.189990	-0.043084	4.291959
207.965432	6315.550051	8.194995	-0.043104	4.294592
208.403715	6323.566231	8.200000	-0.043191	4.297225
208.441181	6331.547715	8.205005	-0.043203	4.299843
208.573001	6339.577557	8.210010	-0.043233	4.302475
208.606583	6347.620446	8.215014	-0.043245	4.305110
208.728385	6355.578411	8.220019	-0.043273	4.307715
209.041071	6363.617920	8.225024	-0.043337	4.310347
209.213566	6371.665743	8.230029	-0.043374	4.312980
209.325664	6379.694146	8.235034	-0.043401	4.315603
209.302049	6387.678946	8.240038	-0.043402	4.318210
209.401929	6395.680120	8.245043	-0.043426	4.320822
209.679059	6403.698473	8.250048	-0.043483	4.323439
209.956160	6411.694972	8.255053	-0.043540	4.326047
209.901937	6419.712378	8.260058	-0.043535	4.328658
210.162499	6427.786231	8.265062	-0.043589	4.331288
210.255121	6435.794834	8.270067	-0.043612	4.333894
210.470857	6443.831587	8.275072	-0.043657	4.336508
210.616976	6451.772888	8.280077	-0.043690	4.339089
211.053861	6459.866712	8.285082	-0.043777	4.341720
211.094722	6467.806484	8.290086	-0.043790	4.344297
211.223496	6475.823312	8.295091	-0.043819	4.346898
211.450861	6483.868025	8.300096	-0.043867	4.349507
211.600679	6491.927924	8.305101	-0.043900	4.352119
211.653281	6500.015917	8.310106	-0.043916	4.354738
211.910454	6508.040049	8.315110	-0.043969	4.357336
212.245703	6515.935220	8.320115	-0.044037	4.359891
212.140099	6523.969432	8.325120	-0.044022	4.362486
212.301932	6531.912312	8.330125	-0.044058	4.365053
212.653076	6540.004335	8.335130	-0.044129	4.367667
212.869398	6548.008075	8.340134	-0.044175	4.370250
212.861713	6556.022797	8.345139	-0.044179	4.372834
213.123189	6564.067300	8.350144	-0.044233	4.375427
213.345782	6572.053394	8.355149	-0.044280	4.378000
213.586764	6580.047829	8.360154	-0.044330	4.380574
213.747401	6588.085419	8.365158	-0.044365	4.383160
213.644263	6596.103386	8.370163	-0.044351	4.385737
214.057316	6604.149979	8.375168	-0.044434	4.388324
213.949723	6612.130816	8.380173	-0.044419	4.390885
214.236361	6620.187339	8.385178	-0.044478	4.393472
214.612590	6628.208250	8.390182	-0.044554	4.396046
214.643169	6636.173586	8.395187	-0.044565	4.398599
214.652987	6644.224843	8.400192	-0.044572	4.401178
214.915998	6652.152760	8.405197	-0.044626	4.403717
215.055923	6660.217201	8.410202	-0.044658	4.406298
215.267224	6668.278449	8.415206	-0.044703	4.408876
215.464007	6676.273393	8.420211	-0.044745	4.411432
215.766353	6684.325188	8.425216	-0.044806	4.414005
215.844280	6692.355934	8.430221	-0.044826	4.416568
216.011431	6700.298967	8.435226	-0.044863	4.419102
216.147040	6708.398953	8.440230	-0.044894	4.421685
216.241128	6716.340663	8.445235	-0.044916	4.424216
216.776802	6724.428559	8.450240	-0.045022	4.426794
216.887100	6732.409810	8.455245	-0.045048	4.429334
216.796520	6740.484983	8.460250	-0.045036	4.431902
216.926610	6748.530251	8.465254	-0.045066	4.434460
217.096568	6756.464652	8.470259	-0.045103	4.436981
217.506854	6764.485911	8.475264	-0.045185	4.439530
217.616464	6772.468785	8.480269	-0.045211	4.442063
217.719526	6780.436659	8.485274	-0.045235	4.444590
217.704525	6788.527925	8.490278	-0.045238	4.447155
217.822852	6796.535376	8.495283	-0.045265	4.449692
218.037762	6804.613297	8.500288	-0.045311	4.452250
218.183608	6812.603058	8.505293	-0.045343	4.454779
218.533701	6820.628473	8.510298	-0.045414	4.457318
218.766447	6828.625457	8.515302	-0.045463	4.459846
218.823795	6836.630171	8.520307	-0.045479	4.462374
219.133058	6844.629557	8.525312	-0.045542	4.464901
218.923554	6852.670312	8.530317	-0.045508	4.467437
219.068010	6860.697655	8.535322	-0.045541	4.469968
219.282799	6868.742700	8.540326	-0.045586	4.472504
219.465308	6876.706494	8.545331	-0.045625	4.475013
219.751421	6884.733243	8.550336	-0.045684	4.477541
219.714342	6892.755180	8.555341	-0.045683	4.480064
219.935702	6900.749138	8.560346	-0.045729	4.482578
220.192714	6908.744333	8.565351	-0.045783	4.485092
220.159223	6916.773890	8.570355	-0.045782	4.487613
220.397255	6924.810256	8.575360	-0.045832	4.490136
220.515897	6932.862354	8.580365	-0.045859	4.492663
220.576183	6940.850863	8.585370	-0.045876	4.495168
220.926835	6948.889006	8.590375	-0.045947	4.497687
221.206725	6956.799819	8.595379	-0.046004	4.500166
221.191524	6964.873379	8.600384	-0.046007	4.502693
221.350799	6972.851130	8.605389	-0.046042	4.505189
221.494670	6980.933392	8.610394	-0.046074	4.507716
221.673192	6988.951007	8.615399	-0.046113	4.510222
221.734611	6997.005107	8.620403	-0.046130	4.512737
222.058839	7005.032640	8.625408	-0.046195	4.515243
222.170838	7013.014349	8.630413	-0.046222	4.517733
222.172056	7021.000344	8.635418	-0.046227	4.520223
222.447543	7029.023820	8.640423	-0.046284	4.522724
222.568002	7036.968725	8.645427	-0.046312	4.525198
222.728325	7045.036150	8.650432	-0.046347	4.527710
222.938741	7053.013422	8.655437	-0.046392	4.530192
223.190422	7061.057165	8.660442	-0.046444	4.532693
223.366253	7069.109961	8.665447	-0.046482	4.535196
223.260446	7077.052370	8.670451	-0.046468	4.537662
223.722147	7085.114405	8.675456	-0.046559	4.540165
223.842848	7093.154859	8.680461	-0.046587	4.542660
224.058044	7101.113646	8.685466	-0.046633	4.545128
224.329093	7109.170275	8.690471	-0.046689	4.547625
224.565453	7117.160034	8.695475	-0.046738	4.550099
224.829420	7125.248944	8.700480	-0.046793	4.552604
224.652191	7133.252671	8.705485	-0.046765	4.555079
225.184996	7141.269548	8.710490	-0.046870	4.557559
225.274659	7149.255567	8.715495	-0.046892	4.560027
225.271673	7157.215000	8.720499	-0.046897	4.562485
225.529669	7165.228269	8.725504	-0.046950	4.564959
225.690078	7173.278758	8.730509	-0.046985	4.567443
225.861452	7181.257701	8.735514	-0.047023	4.569903
225.987585	7189.377976	8.740519	-0.047052	4.572406
226.161259	7197.321117	8.745523	-0.047090	4.574853
226.210013	7205.385625	8.750528	-0.047104	4.577335
226.174510	7213.361399	8.755533	-0.047103	4.579789
226.412322	7221.422980	8.760538	-0.047153	4.582268
226.834543	7229.395095	8.765543	-0.047237	4.584719
226.855573	7237.431520	8.770547	-0.047246	4.587187
226.971188	7245.450733	8.775552	-0.047273	4.589649
227.157994	7253.496563	8.780557	-0.047313	4.592118
227.487052	7261.513981	8.785562	-0.047380	4.594577
227.458828	7269.543491	8.790567	-0.047380	4.597038
227.707379	7277.448501	8.795571	-0.047432	4.599460
227.781197	7285.552781	8.800576	-0.047451	4.601941
227.807257	7293.514564	8.805581	-0.047461	4.604378
228.139424	7301.556945	8.810586	-0.047528	4.606838
228.361423	7309.562955	8.815591	-0.047575	4.609285
228.274880	7317.592830	8.820595	-0.047565	4.611738
228.879673	7325.648354	8.825600	-0.047683	4.614198
228.969597	7333.679727	8.830605	-0.047705	4.616649
229.090638	7341.607923	8.835610	-0.047733	4.619067
229.316375	7349.706320	8.840615	-0.047780	4.621536
229.388943	7357.651209	8.845619	-0.047799	4.623957
229.584914	7365.728582	8.850624	-0.047841	4.626417
229.716581	7373.674842	8.855629	-0.047871	4.628835
229.849947	7381.726945	8.860634	-0.047901	4.631285
230.081869	7389.802000	8.865639	-0.047950	4.633740
230.070526	7397.769028	8.870643	-0.047953	4.636161
230.474880	7405.740986	8.875648	-0.048034	4.638582
230.299275	7413.752102	8.880653	-0.048007	4.641014
230.531435	7421.744594	8.885658	-0.048055	4.643439
230.609408	7429.806896	8.890663	-0.048075	4.645884
230.580429	7437.752656	8.895667	-0.048075	4.648292
230.757670	7445.844340	8.900672	-0.048114	4.650744
231.065069	7453.874750	8.905677	-0.048176	4.653175
231.089430	7461.895168	8.910682	-0.048186	4.655602
231.295185	7469.879103	8.915687	-0.048230	4.658016
231.352084	7477.877066	8.920691	-0.048246	4.660434
231.555112	7485.936611	8.925696	-0.048289	4.662869
231.729345	7493.907270	8.930701	-0.048327	4.665275
231.889560	7501.930692	8.935706	-0.048363	4.667697
232.086037	7509.960578	8.940711	-0.048405	4.670119
232.159559	7518.014873	8.945715	-0.048424	4.672547
232.558442	7526.127792	8.950720	-0.048503	4.674991
232.639675	7534.067285	8.955725	-0.048524	4.677383
232.630762	7542.050874	8.960730	-0.048528	4.679786
232.827449	7550.065617	8.965735	-0.048570	4.682197
233.036128	7557.977681	8.970739	-0.048614	4.684576
233.297632	7566.029225	8.975744	-0.048668	4.686996
233.381482	7574.051763	8.980749	-0.048689	4.689405
233.361380	7582.080952	8.985754	-0.048691	4.691816
233.566597	7590.136505	8.990759	-0.048735	4.694233
233.651829	7598.138255	8.995763	-0.048756	4.696633
233.901601	7606.083781	9.000768	-0.048808	4.699015
233.782871	7614.133039	9.005773	-0.048791	4.701427
234.005844	7622.100182	9.010778	-0.048838	4.703812
234.188691	7630.192191	9.015783	-0.048878	4.706234
234.382664	7638.159097	9.020787	-0.048919	4.708617
234.566882	7646.188531	9.025792	-0.048959	4.711018
234.796289	7654.286234	9.030797	-0.049007	4.713437
234.753836	7662.249051	9.035802	-0.049005	4.715816
235.213281	7670.267092	9.040807	-0.049095	4.718208
235.324448	7678.277027	9.045811	-0.049122	4.720598
235.366693	7686.285240	9.050816	-0.049135	4.722987
235.588752	7694.311693	9.055821	-0.049182	4.725379
235.721469	7702.332066	9.060826	-0.049212	4.727768
235.789212	7710.330788	9.065831	-0.049230	4.730150
235.758727	7718.392453	9.070835	-0.049230	4.732549
235.789317	7726.422054	9.075840	-0.049241	4.734938
236.028001	7734.451471	9.080845	-0.049291	4.737325
236.264033	7742.430371	9.085850	-0.049340	4.739695
236.521867	7750.497691	9.090855	-0.049394	4.742091
236.384048	7758.416773	9.095859	-0.049373	4.744442
236.749466	7766.457674	9.100864	-0.049447	4.746827
236.791342	7774.474006	9.105869	-0.049460	4.749205
236.990492	7782.481360	9.110874	-0.049502	4.751578
237.186023	7790.564431	9.115879	-0.049544	4.753972
237.271069	7798.567097	9.120883	-0.049566	4.756342
237.388057	7806.545679	9.125888	-0.049593	4.758703
237.516725	7814.510469	9.130893	-0.049622	4.761059
237.653034	7822.522653	9.135898	-0.049653	4.763427
237.887237	7830.574943	9.140903	-0.049702	4.765806
238.033441	7838.544639	9.145907	-0.049735	4.768160
237.956265	7846.592746	9.150912	-0.049726	4.770536
238.203844	7854.625701	9.155917	-0.049777	4.772906
238.430312	7862.627539	9.160922	-0.049825	4.775265
238.582945	7870.623986	9.165927	-0.049859	4.777622
238.563289	7878.623214	9.170931	-0.049860	4.779979
238.679100	7886.668513	9.175936	-0.049887	4.782348
238.994438	7894.668608	9.180941	-0.049952	4.784702
239.095748	7902.695269	9.185946	-0.049976	4.787063
239.130201	7910.729244	9.190951	-0.049988	4.789425
239.095909	7918.755601	9.195955	-0.049987	4.791785
239.548517	7926.818475	9.200960	-0.050077	4.794151
239.426474	7934.788807	9.205965	-0.050059	4.796492
239.652491	7942.702204	9.210970	-0.050107	4.798814
239.950614	7950.815423	9.215975	-0.050168	4.801193
239.973226	7958.759236	9.220979	-0.050177	4.803522
240.022544	7966.850123	9.225984	-0.050192	4.805892
240.199103	7974.829753	9.230989	-0.050230	4.808229
240.221445	7982.827960	9.235994	-0.050240	4.810570
240.300008	7990.317687	9.240999	-0.050260	4.812762
240.275707	7994.793460	9.246003	-0.050258	4.814071

240.653744	7997.177983	9.251008	-0.050330	4.814767
240.721053	7998.511491	9.256013	-0.050344	4.815156
240.589172	7998.970608	9.261018	-0.050320	4.815291
240.646913	7999.804391	9.266023	-0.050331	4.815535
240.914429	7999.805557	9.271027	-0.050381	4.815534
240.883119	7999.824285	9.276032	-0.050376	4.815539
241.004551	7999.811330	9.281037	-0.050399	4.815535
241.130369	7999.825140	9.286042	-0.050422	4.815538
241.175160	7999.837633	9.291047	-0.050431	4.815542
241.161502	7999.745601	9.296051	-0.050428	4.815515
241.510054	7999.813220	9.301056	-0.050494	4.815533
241.348500	7999.805271	9.306061	-0.050464	4.815532
241.229744	7999.755307	9.311066	-0.050442	4.815518
241.409779	7999.825524	9.316071	-0.050475	4.815537
241.238652	7999.798199	9.321075	-0.050444	4.815530
241.318555	7999.861448	9.326080	-0.050459	4.815548
241.153816	7999.797923	9.331085	-0.050428	4.815530
241.330920	7999.777332	9.336090	-0.050462	4.815523
241.381014	7999.801656	9.341095	-0.050471	4.815530
241.344097	7999.790395	9.346099	-0.050464	4.815527
241.524749	7999.841403	9.351104	-0.050498	4.815541
241.574926	7999.842237	9.356109	-0.050508	4.815541
241.412354	7999.773408	9.361114	-0.050478	4.815522
241.581509	7999.800737	9.366119	-0.050510	4.815529
241.520151	7999.804028	9.371123	-0.050498	4.815530
241.660243	7999.811665	9.376128	-0.050525	4.815532
241.598199	7999.823487	9.381133	-0.050513	4.815536
241.610263	7999.807684	9.386138	-0.050516	4.815531
241.693299	7999.933984	9.391143	-0.050531	4.815567
241.642565	7999.843483	9.396147	-0.050522	4.815541
241.543300	7999.846157	9.401152	-0.050504	4.815542
241.748011	7999.849506	9.406157	-0.050542	4.815542
241.731704	7999.840717	9.411162	-0.050539	4.815540
241.728993	7999.899419	9.416167	-0.050539	4.815557
241.751821	7999.929707	9.421171	-0.050544	4.815566
241.717340	7999.903537	9.426176	-0.050537	4.815558
241.632689	7999.870144	9.431181	-0.050522	4.815549
241.819340	7999.861454	9.436186	-0.050557	4.815546
241.900391	7999.865994	9.441191	-0.050572	4.815547
241.787549	7999.885532	9.446195	-0.050551	4.815553
242.118858	7999.826874	9.451200	-0.050613	4.815534
242.049154	7999.841775	9.456205	-0.050600	4.815539
242.074137	7999.899861	9.461210	-0.050605	4.815556
242.120582	7999.844042	9.466215	-0.050614	4.815539
242.138619	7999.828336	9.471219	-0.050618	4.815534
242.264415	7999.803707	9.476224	-0.050641	4.815527
242.004384	7999.892391	9.481229	-0.050593	4.815554
242.207059	7999.781454	9.486234	-0.050631	4.815520
242.302475	7999.926110	9.491239	-0.050649	4.815562
242.175560	7999.796995	9.496243	-0.050626	4.815525
242.026416	7999.828755	9.501248	-0.050598	4.815535
242.275843	7999.908646	9.506253	-0.050645	4.815557
242.221714	7999.829834	9.511258	-0.050635	4.815534
242.185460	7999.846347	9.516263	-0.050628	4.815539
242.112511	7999.845178	9.521267	-0.050615	4.815539
242.182291	7999.889044	9.526272	-0.050628	4.815552
242.162005	7999.841749	9.531277	-0.050625	4.815538
242.089663	7999.787200	9.536282	-0.050611	4.815523
242.349295	7999.937732	9.541287	-0.050660	4.815565
242.307007	7999.799316	9.546291	-0.050652	4.815525
242.270630	7999.895911	9.551296	-0.050646	4.815553
242.177820	7999.843165	9.556301	-0.050628	4.815538
242.208967	7999.854368	9.561306	-0.050635	4.815542
242.288267	7999.887711	9.566311	-0.050650	4.815551
242.236968	7999.861267	9.571315	-0.050640	4.815543
242.621944	7999.844059	9.576320	-0.050712	4.815537
242.340424	7999.859783	9.581325	-0.050660	4.815542
242.220459	7999.885612	9.586330	-0.050638	4.815551
242.457000	7999.874531	9.591335	-0.050682	4.815546
242.408205	7999.799009	9.596339	-0.050673	4.815524
242.499020	7999.805844	9.601344	-0.050690	4.815526
242.776223	7999.943851	9.606349	-0.050742	4.815565
242.699703	7999.787791	9.611354	-0.050728	4.815520
242.525991	7999.870406	9.616359	-0.050696	4.815545
242.486619	7999.819596	9.621363	-0.050689	4.815530
242.526100	7999.852291	9.626368	-0.050696	4.815539
242.584278	7999.812680	9.631373	-0.050707	4.815528
242.587454	7999.918463	9.636378	-0.050708	4.815558
242.660302	7999.908989	9.641383	-0.050722	4.815555
242.676078	7999.805686	9.646387	-0.050725	4.815525
242.398132	7999.870588	9.651392	-0.050673	4.815545
242.606403	7999.867589	9.656397	-0.050712	4.815543
242.726001	7999.847130	9.661402	-0.050735	4.815537
242.681431	7999.881661	9.666407	-0.050727	4.815547
242.674262	7999.806815	9.671411	-0.050726	4.815525
242.519614	7999.861978	9.676416	-0.050697	4.815542
242.558597	7999.887190	9.681421	-0.050705	4.815549
242.868283	7999.958455	9.686426	-0.050763	4.815569
242.786469	7999.878122	9.691431	-0.050747	4.815546
242.625876	7999.827475	9.696435	-0.050718	4.815532
242.685450	7999.838073	9.701440	-0.050729	4.815534
242.693589	7999.865987	9.706445	-0.050731	4.815542
242.890947	7999.882032	9.711450	-0.050768	4.815546
243.034784	7999.807509	9.716455	-0.050795	4.815524
242.788989	7999.855848	9.721459	-0.050749	4.815539
242.813714	7999.890439	9.726464	-0.050754	4.815549
242.658211	7999.860163	9.731469	-0.050725	4.815541
242.433564	7999.817015	9.736474	-0.050684	4.815529
242.786037	7999.856941	9.741479	-0.050749	4.815539
242.708216	7999.885591	9.746483	-0.050735	4.815548
242.790843	7999.754546	9.751488	-0.050751	4.815509
242.736124	7999.964032	9.756493	-0.050741	4.815571
242.701172	7999.795835	9.761498	-0.050734	4.815522
242.798196	7999.817721	9.766503	-0.050753	4.815528
242.536735	7999.903179	9.771507	-0.050704	4.815554
242.789851	7999.827232	9.776512	-0.050752	4.815531
242.818572	7999.850141	9.781517	-0.050757	4.815537
242.892659	7999.875925	9.786522	-0.050771	4.815544
242.974953	7999.787587	9.791527	-0.050787	4.815518
243.083291	7999.900422	9.796531	-0.050807	4.815551
243.096140	7999.824834	9.801536	-0.050810	4.815528
243.184197	7999.856185	9.806541	-0.050826	4.815537
243.080078	7999.875864	9.811546	-0.050807	4.815543
242.854133	7999.792118	9.816551	-0.050765	4.815520
242.816015	7999.861991	9.821555	-0.050758	4.815541
243.186867	7999.778350	9.826560	-0.050828	4.815514
243.064889	7999.885300	9.831565	-0.050805	4.815546
242.910532	7999.834753	9.836570	-0.050777	4.815532
242.955948	7999.825901	9.841575	-0.050785	4.815529
242.928241	7999.803044	9.846579	-0.050780	4.815523
243.055160	7999.839298	9.851584	-0.050804	4.815533
243.127765	7999.861855	9.856589	-0.050818	4.815539
243.060804	7999.849037	9.861594	-0.050806	4.815536
243.105502	7999.888224	9.866599	-0.050814	4.815547
242.947848	7999.836556	9.871603	-0.050785	4.815532
242.922633	7999.790248	9.876608	-0.050780	4.815519
243.030354	7999.937243	9.881613	-0.050801	4.815562
242.931922	7999.784028	9.886618	-0.050783	4.815517
242.966557	7999.854018	9.891623	-0.050789	4.815537
243.101398	7999.819926	9.896627	-0.050815	4.815527
242.994499	7999.915376	9.901632	-0.050795	4.815555
242.826085	7999.853922	9.906637	-0.050764	4.815538
243.006153	7999.817362	9.911642	-0.050797	4.815527
243.071748	7999.873975	9.916647	-0.050810	4.815543
242.961454	7999.868994	9.921651	-0.050790	4.815542
243.049972	7999.858707	9.926656	-0.050806	4.815538
243.218921	7999.870019	9.931661	-0.050838	4.815541
243.188479	7999.820422	9.936666	-0.050832	4.815527
243.166386	7999.855318	9.941671	-0.050829	4.815537
243.106300	7999.846883	9.946675	-0.050818	4.815535
243.222885	7999.826376	9.951680	-0.050840	4.815528
243.136086	7999.867693	9.956685	-0.050824	4.815541
243.124577	7999.887813	9.961690	-0.050822	4.815547
243.322380	7999.873967	9.966695	-0.050859	4.815542
243.231172	7999.857550	9.971699	-0.050842	4.815537
243.406555	7999.827322	9.976704	-0.050875	4.815528
243.385925	7999.840886	9.981709	-0.050871	4.815532
243.093226	7999.787018	9.986714	-0.050817	4.815517
243.152886	7999.930028	9.991719	-0.050828	4.815559
243.268614	7999.832623	9.996723	-0.050850	4.815530
243.456650	7999.825025	10.001728	-0.050885	4.815527
243.411964	7999.847807	10.006733	-0.050877	4.815533
243.429885	7999.805404	10.011738	-0.050881	4.815521
243.453685	7999.849591	10.016743	-0.050885	4.815534
243.309930	7999.883574	10.021747	-0.050859	4.815544
243.274410	7999.937474	10.026752	-0.050852	4.815560
243.359177	7999.875870	10.031757	-0.050868	4.815542
243.174566	7999.801338	10.036762	-0.050834	4.815521
243.364114	7999.855698	10.041767	-0.050870	4.815536
243.194084	7999.829456	10.046771	-0.050838	4.815529
243.297238	7999.806593	10.051776	-0.050857	4.815522
243.546757	7999.852320	10.056781	-0.050904	4.815534
243.297549	7999.842941	10.061786	-0.050858	4.815532
243.273371	7999.837226	10.066791	-0.050854	4.815531
243.230702	7999.785294	10.071795	-0.050846	4.815516
243.266946	7999.784835	10.076800	-0.050853	4.815516
243.581217	7999.953349	10.081805	-0.050912	4.815563
243.413578	7999.820361	10.086810	-0.050881	4.815525
243.344473	7999.881188	10.091815	-0.050868	4.815543
243.154679	7999.835403	10.096819	-0.050833	4.815531
243.358616	7999.805639	10.101824	-0.050871	4.815521
243.498846	7999.863468	10.106829	-0.050897	4.815537
243.394821	7999.878877	10.111834	-0.050878	4.815542
243.326389	7999.784880	10.116839	-0.050866	4.815515
243.308814	7999.951193	10.121843	-0.050863	4.815564
243.333699	7999.842698	10.126848	-0.050867	4.815532
243.593322	7999.801027	10.131853	-0.050916	4.815519
243.425235	7999.848496	10.136858	-0.050885	4.815533
243.492106	7999.877367	10.141863	-0.050898	4.815542
243.423581	7999.854913	10.146867	-0.050885	4.815535
243.334316	7999.912208	10.151872	-0.050869	4.815552
243.310288	7999.848833	10.156877	-0.050864	4.815534
243.195406	7999.844845	10.161882	-0.050843	4.815533
243.420057	7999.802605	10.166887	-0.050885	4.815520
243.440807	7999.924694	10.171891	-0.050889	4.815556
243.507738	7999.794458	10.176896	-0.050902	4.815517
243.525057	7999.841743	10.181901	-0.050905	4.815531
243.458620	7999.813984	10.186906	-0.050893	4.815523
243.624257	7999.828445	10.191911	-0.050924	4.815527
243.778727	7999.934560	10.196915	-0.050953	4.815557
243.776450	7999.832028	10.201920	-0.050953	4.815527
243.603568	7999.864469	10.206925	-0.050921	4.815537
243.354970	7999.808115	10.211930	-0.050875	4.815522
243.495930	7999.852074	10.216935	-0.050901	4.815534
243.551727	7999.871154	10.221939	-0.050912	4.815539
243.454401	7999.814060	10.226944	-0.050894	4.815523
243.451772	7999.938972	10.231949	-0.050894	4.815560
243.417445	7999.816698	10.236954	-0.050888	4.815524
243.417342	7999.863699	10.241959	-0.050888	4.815538
243.336284	7999.851719	10.246963	-0.050873	4.815535
243.459071	7999.885772	10.251968	-0.050896	4.815544
243.450301	7999.841866	10.256973	-0.050895	4.815531
243.318413	7999.793820	10.261978	-0.050870	4.815518
243.439699	7999.852408	10.266983	-0.050893	4.815534
243.345067	7999.856225	10.271987	-0.050876	4.815536
243.431635	7999.879009	10.276992	-0.050892	4.815542
243.507795	7999.791638	10.281997	-0.050906	4.815516
243.411857	7999.869113	10.287002	-0.050889	4.815539
243.459361	7999.795157	10.292007	-0.050898	4.815518
243.556128	7999.957994	10.297011	-0.050916	4.815565
243.440017	7999.818370	10.302016	-0.050894	4.815524
243.625935	7999.869469	10.307021	-0.050929	4.815538
243.557039	7999.848076	10.312026	-0.050917	4.815532
243.673037	7999.830762	10.317031	-0.050939	4.815527
243.756708	7999.835347	10.322035	-0.050954	4.815528
243.657189	7999.888204	10.327040	-0.050936	4.815544
243.520185	7999.894533	10.332045	-0.050911	4.815546
243.512586	7999.852782	10.337050	-0.050909	4.815534
243.558343	7999.873834	10.342055	-0.050918	4.815540
243.605556	7999.853265	10.347059	-0.050927	4.815534
243.668382	7999.862849	10.352064	-0.050939	4.815536
243.637648	7999.889062	10.357069	-0.050934	4.815544
243.538180	7999.822323	10.362074	-0.050915	4.815525
243.725108	7999.884116	10.367079	-0.050950	4.815542
243.852970	7999.853114	10.372083	-0.050974	4.815532
243.684848	7999.872819	10.377088	-0.050943	4.815539
243.788294	7999.863843	10.382093	-0.050963	4.815536
243.807783	7999.830008	10.387098	-0.050967	4.815526
243.603962	7999.876895	10.392103	-0.050929	4.815541
243.573958	7999.844389	10.397107	-0.050923	4.815531
243.709839	7999.790025	10.402112	-0.050949	4.815515
243.777115	7999.868023	10.407117	-0.050962	4.815537
243.691880	7999.851704	10.412122	-0.050946	4.815533
243.820441	7999.830323	10.417127	-0.050970	4.815526
243.571181	7999.835892	10.422131	-0.050924	4.815529
243.643846	7999.923589	10.427136	-0.050938	4.815554
243.694849	7999.860367	10.432141	-0.050947	4.815535
243.618805	7999.807891	10.437146	-0.050933	4.815520
243.865645	7999.818336	10.442151	-0.050980	4.815522
243.818504	7999.823994	10.447155	-0.050971	4.815524
243.759938	7999.875382	10.452160	-0.050960	4.815539
243.754794	7999.850756	10.457165	-0.050960	4.815532
243.805308	7999.882565	10.462170	-0.050969	4.815541
243.674932	7999.829203	10.467175	-0.050945	4.815526
243.711045	7999.843691	10.472179	-0.050952	4.815530
243.607667	7999.861247	10.477184	-0.050933	4.815536
243.618147	7999.788823	10.482189	-0.050935	4.815515
243.632876	7999.767724	10.487194	-0.050938	4.815508
243.811717	7999.879575	10.492199	-0.050972	4.815540
243.798508	7999.771526	10.497203	-0.050969	4.815509
243.899001	7999.902390	10.502208	-0.050988	4.815547
244.127122	7999.864478	10.507213	-0.051031	4.815534
243.822937	7999.813624	10.512218	-0.050975	4.815521
243.886048	7999.839230	10.517223	-0.050986	4.815528
244.039260	7999.840676	10.522227	-0.051015	4.815528
243.979309	7999.808751	10.527232	-0.051004	4.815519
244.081520	7999.942847	10.532237	-0.051024	4.815557
243.925913	7999.830342	10.537242	-0.050995	4.815525
243.872549	7999.877544	10.542247	-0.050985	4.815539
244.001031	7999.863637	10.547251	-0.051009	4.815535
244.081686	7999.854291	10.552256	-0.051024	4.815532
244.110276	7999.907100	10.557261	-0.051030	4.815547
243.921216	7999.861324	10.562266	-0.050995	4.815534
243.982863	7999.900789	10.567271	-0.051007	4.815546
244.083150	7999.896034	10.572275	-0.051026	4.815544
243.860558	7999.894562	10.577280	-0.050984	4.815544
243.869164	7999.878702	10.582285	-0.050986	4.815540
243.916964	7999.832514	10.587290	-0.050995	4.815526
244.013737	7999.896044	10.592295	-0.051013	4.815544
243.781358	7999.831409	10.597299	-0.050970	4.815526
243.728616	7999.925606	10.602304	-0.050961	4.815554
244.003916	7999.888463	10.607309	-0.051012	4.815542
243.800736	7999.864883	10.612314	-0.050975	4.815536
243.896817	7999.856855	10.617319	-0.050993	4.815533
243.945743	7999.863010	10.622323	-0.051002	4.815535
243.933687	7999.822253	10.627328	-0.051000	4.815523
243.991626	7999.850979	10.632333	-0.051011	4.815531
243.906073	7999.835722	10.637338	-0.050995	4.815527
244.140312	7999.853438	10.642343	-0.051039	4.815531
244.043742	7999.879647	10.647347	-0.051021	4.815539
243.876896	7999.841708	10.652352	-0.050990	4.815529
243.959134	7999.851609	10.657357	-0.051006	4.815531
243.823845	7999.936987	10.662362	-0.050981	4.815557
243.999934	7999.839496	10.667367	-0.051014	4.815528
244.038674	7999.866841	10.672371	-0.051021	4.815535
243.911457	7999.876533	10.677376	-0.050998	4.815539
243.900209	7999.926557	10.682381	-0.050996	4.815553
244.061015	7999.824546	10.687386	-0.051026	4.815523
244.047608	7999.840363	10.692391	-0.051024	4.815528
243.962890	7999.856087	10.697395	-0.051008	4.815532
243.770742	7999.891418	10.702400	-0.050973	4.815544
244.010692	7999.901752	10.707405	-0.051018	4.815546
243.948559	7999.871926	10.712410	-0.051006	4.815537
243.849956	7999.879948	10.717415	-0.050988	4.815540
244.112578	7999.962198	10.722419	-0.051037	4.815563
243.956409	7999.852887	10.727424	-0.051008	4.815532
244.073261	7999.868691	10.732429	-0.051030	4.815536
244.223307	7999.794268	10.737434	-0.051058	4.815513
243.972811	7999.838259	10.742439	-0.051012	4.815527
243.942504	7999.892244	10.747443	-0.051007	4.815543
243.950597	7999.835798	10.752448	-0.051008	4.815527
244.127772	7999.899570	10.757453	-0.051042	4.815544
243.928379	7999.871779	10.762458	-0.051005	4.815537
244.047263	7999.883344	10.767463	-0.051027	4.815540
244.040285	7999.881113	10.772467	-0.051026	4.815539
244.047540	7999.884453	10.777472	-0.051027	4.815540
244.173624	7999.874779	10.782477	-0.051051	4.815537
244.170980	7999.832040	10.787482	-0.051051	4.815524
244.031424	7999.834056	10.792487	-0.051025	4.815526
244.091904	7999.892724	10.797491	-0.051037	4.815542
243.848357	7999.822568	10.802496	-0.050991	4.815523
244.195195	7999.856000	10.807501	-0.051056	4.815531
244.000876	7999.822953	10.812506	-0.051020	4.815523
244.086306	7999.923673	10.817511	-0.051036	4.815552
244.321193	7999.898686	10.822515	-0.051080	4.815543
244.338690	7999.812493	10.827520	-0.051084	4.815518
244.202136	7999.855136	10.832525	-0.051058	4.815531
243.843223	7999.864258	10.837530	-0.050992	4.815535
244.076908	7999.845658	10.842535	-0.051036	4.815529
243.991599	7999.843218	10.847539	-0.051020	4.815528
243.981178	7999.844135	10.852544	-0.051018	4.815529
244.129866	7999.873271	10.857549	-0.051046	4.815537
243.916020	7999.858059	10.862554	-0.051006	4.815533
243.880024	7999.808370	10.867559	-0.051000	4.815519
244.034423	7999.919824	10.872563	-0.051029	4.815551
243.944098	7999.785958	10.877568	-0.051012	4.815512
244.195294	7999.786864	10.882573	-0.051059	4.815511
244.060809	7999.784692	10.887578	-0.051034	4.815511
244.207495	7999.914174	10.892583	-0.051062	4.815548
244.023240	7999.850323	10.897587	-0.051028	4.815530
243.874654	7999.850056	10.902592	-0.051000	4.815531
244.211996	7999.871588	10.907597	-0.051063	4.815536
244.093222	7999.826957	10.912602	-0.051041	4.815523
244.298521	7999.827116	10.917607	-0.051080	4.815522
244.329458	7999.823367	10.922611	-0.051086	4.815521
244.209800	7999.821435	10.927616	-0.051064	4.815521
244.148060	7999.836466	10.932621	-0.051053	4.815526
244.245137	7999.865830	10.937626	-0.051071	4.815534
244.350173	7999.829116	10.942631	-0.051091	4.815523
244.286180	7999.851585	10.947635	-0.051079	4.815529
244.205623	7999.778744	10.952640	-0.051064	4.815508
244.115947	7999.946023	10.957645	-0.051048	4.815558
244.339583	7999.834356	10.962650	-0.051089	4.815524
244.248668	7999.816875	10.967655	-0.051073	4.815519
244.078892	7999.852570	10.972659	-0.051041	4.815531
244.238032	7999.822077	10.977664	-0.051071	4.815521
244.247911	7999.884192	10.982669	-0.051073	4.815539
244.122026	7999.842649	10.987674	-0.051050	4.815528
244.096684	7999.855068	10.992679	-0.051045	4.815531
244.259889	7999.920749	10.997683	-0.051076	4.815550
244.165803	7999.813517	11.002688	-0.051059	4.815519
244.345520	7999.854905	11.007693	-0.051092	4.815530
244.474567	7999.776937	11.012698	-0.051117	4.815507
244.299111	7999.863796	11.017703	-0.051084	4.815533
244.103916	7999.848888	11.022707	-0.051048	4.815529
244.269632	7999.825978	11.027712	-0.051079	4.815522
244.213446	7999.870998	11.032717	-0.051069	4.815535
244.031814	7999.843497	11.037722	-0.051035	4.815528
244.256342	7999.791644	11.042727	-0.051077	4.815512
244.303768	7999.956885	11.047731	-0.051086	4.815560
244.133618	7999.785410	11.052736	-0.051055	4.815511
244.232951	7999.813743	11.057741	-0.051074	4.815518
244.129693	7999.834504	11.062746	-0.051055	4.815525
244.132655	7999.769431	11.067751	-0.051055	4.815506
244.340346	7999.916994	11.072755	-0.051094	4.815548
244.221160	7999.787995	11.077760	-0.051072	4.815511
244.140416	7999.835819	11.082765	-0.051057	4.815525
244.096303	7999.844729	11.087770	-0.051049	4.815528
244.260735	7999.814323	11.092775	-0.051080	4.815518
244.261538	7999.872018	11.097779	-0.051081	4.815535
244.289982	7999.787071	11.102784	-0.051086	4.815510
244.344025	7999.843498	11.107789	-0.051096	4.815527
244.142861	7999.819950	11.112794	-0.051059	4.815521
244.191193	7999.838909	11.117799	-0.051068	4.815526
244.371650	7999.840800	11.122803	-0.051102	4.815526
244.170255	7999.816180	11.127808	-0.051065	4.815519
244.317618	7999.886941	11.132813	-0.051092	4.815539
244.250257	7999.906152	11.137818	-0.051080	4.815545
244.024760	7999.798914	11.142823	-0.051038	4.815515
244.353054	7999.853402	11.147827	-0.051100	4.815529
244.394417	7999.887198	11.152832	-0.051108	4.815539
244.222590	7999.842770	11.157837	-0.051076	4.815527
244.224505	7999.837480	11.162842	-0.051076	4.815525
244.273412	7999.789174	11.167847	-0.051086	4.815511
244.313017	7999.883809	11.172851	-0.051093	4.815538
244.323198	7999.822057	11.177856	-0.051095	4.815520
244.381915	7999.882832	11.182861	-0.051107	4.815538
244.340411	7999.894988	11.187866	-0.051099	4.815542
244.352582	7999.765994	11.192871	-0.051101	4.815504
244.439854	7999.916934	11.197875	-0.051118	4.815547
244.367669	7999.877333	11.202880	-0.051105	4.815536
244.545454	7999.826855	11.207885	-0.051138	4.815521
244.380277	7999.768653	11.212890	-0.051107	4.815504
244.624888	7999.914683	11.217895	-0.051153	4.815546
244.427111	7999.851678	11.222899	-0.051117	4.815528
244.276702	7999.818278	11.227904	-0.051089	4.815519
244.529653	7999.841639	11.232909	-0.051136	4.815525
244.276874	7999.804435	11.237914	-0.051089	4.815515
244.156072	7999.792874	11.242919	-0.051067	4.815513
244.565935	7999.888203	11.247923	-0.051143	4.815538
244.639482	7999.761275	11.252928	-0.051157	4.815501
244.652643	7999.843734	11.257933	-0.051160	4.815525
244.530029	7999.893011	11.262938	-0.051137	4.815540
244.761432	7999.905343	11.267943	-0.051181	4.815542
244.564790	7999.900021	11.272947	-0.051144	4.815542
244.505291	7999.910817	11.277952	-0.051133	4.815545
244.673428	7999.884742	11.282957	-0.051165	4.815537
244.543520	7999.854879	11.287962	-0.051141	4.815529
244.607390	7999.820698	11.292967	-0.051153	4.815518
244.580009	7999.824542	11.297971	-0.051148	4.815520
244.616316	7999.805930	11.302976	-0.051155	4.815514
244.630184	7999.851025	11.307981	-0.051158	4.815527
244.424934	7999.849834	11.312986	-0.051120	4.815528
244.524877	7999.831191	11.317991	-0.051139	4.815522
244.341105	7999.936070	11.322995	-0.051105	4.815553
244.250746	7999.781912	11.328000	-0.051088	4.815509
244.380105	7999.847041	11.333005	-0.051112	4.815527
244.501069	7999.847962	11.338010	-0.051135	4.815527
244.318820	7999.817247	11.343015	-0.051101	4.815519
244.509195	7999.859877	11.348019	-0.051137	4.815530
244.447335	7999.864227	11.353024	-0.051126	4.815532
244.474671	7999.833723	11.358029	-0.051131	4.815523
244.526764	7999.855947	11.363034	-0.051141	4.815529
244.645509	7999.862171	11.368039	-0.051163	4.815530
244.518232	7999.844098	11.373043	-0.051140	4.815526
244.200021	7999.781267	11.378048	-0.051081	4.815509
244.443328	7999.850389	11.383053	-0.051126	4.815528
244.434072	7999.937821	11.388058	-0.051125	4.815553
244.322790	7999.848461	11.393063	-0.051104	4.815528
244.384097	7999.910346	11.398067	-0.051116	4.815546
244.332947	7999.878563	11.403072	-0.051107	4.815537
244.365100	7999.841730	11.408077	-0.051113	4.815526
244.408574	7999.848864	11.413082	-0.051121	4.815528
244.596468	7999.814568	11.418087	-0.051156	4.815517
244.755526	7999.844943	11.423091	-0.051186	4.815525
244.677959	7999.868258	11.428096	-0.051172	4.815532
244.809934	7999.904599	11.433101	-0.051197	4.815542
244.423420	7999.895115	11.438106	-0.051125	4.815541
244.399767	7999.866983	11.443111	-0.051121	4.815533
244.294345	7999.877030	11.448115	-0.051101	4.815536
244.325121	7999.747271	11.453120	-0.051107	4.815498
244.312481	7999.865615	11.458125	-0.051105	4.815533
244.420998	7999.800127	11.463130	-0.051125	4.815513
244.595030	7999.848898	11.468135	-0.051158	4.815527
244.474523	7999.820256	11.473139	-0.051136	4.815519
244.408067	7999.865110	11.478144	-0.051124	4.815532
244.504339	7999.795150	11.483149	-0.051142	4.815511
244.721333	7999.807247	11.488154	-0.051182	4.815514
244.563350	7999.864491	11.493159	-0.051153	4.815531
244.519439	7999.830690	11.498163	-0.051145	4.815522
244.536379	7999.821373	11.503168	-0.051149	4.815519
244.572585	7999.771792	11.508173	-0.051155	4.815504
244.459863	7999.906660	11.513178	-0.051135	4.815544
244.373534	7999.783536	11.518183	-0.051119	4.815508
244.439003	7999.831606	11.523187	-0.051131	4.815522
244.260148	7999.863950	11.528192	-0.051098	4.815532
244.384544	7999.790177	11.533197	-0.051121	4.815510
244.420294	7999.870867	11.538202	-0.051128	4.815534
244.498991	7999.814503	11.543207	-0.051143	4.815517
244.308479	7999.966257	11.548211	-0.051108	4.815562
244.264391	7999.810717	11.553216	-0.051100	4.815517
244.338908	7999.855731	11.558221	-0.051114	4.815530
244.482552	7999.829258	11.563226	-0.051141	4.815521
244.534495	7999.834394	11.568231	-0.051151	4.815523
244.462594	7999.870616	11.573235	-0.051138	4.815533
244.491435	7999.851882	11.578240	-0.051143	4.815528
244.439429	7999.885225	11.583245	-0.051134	4.815538
244.335475	7999.850445	11.588250	-0.051115	4.815528
244.450384	7999.829911	11.593255	-0.051136	4.815522
244.650122	7999.876966	11.598259	-0.051174	4.815534
244.424558	7999.803898	11.603264	-0.051132	4.815514
244.686214	7999.832740	11.608269	-0.051181	4.815521
244.505298	7999.960090	11.613274	-0.051147	4.815559
244.552670	7999.774004	11.618279	-0.051156	4.815505
244.499171	7999.784897	11.623283	-0.051147	4.815508
244.220155	7999.938412	11.628288	-0.051095	4.815554
244.358854	7999.834972	11.633293	-0.051121	4.815523
244.357939	7999.837111	11.638298	-0.051121	4.815524
244.355457	7999.853107	11.643303	-0.051121	4.815529
244.141165	7999.852837	11.648307	-0.051081	4.815530
244.282922	7999.863708	11.653312	-0.051108	4.815532
244.301370	7999.812769	11.658317	-0.051111	4.815517
244.256171	7999.787490	11.663322	-0.051103	4.815510
244.522131	7999.754467	11.668327	-0.051153	4.815499
244.381929	7999.978588	11.673331	-0.051127	4.815565
244.245849	7999.833295	11.678336	-0.051102	4.815523
244.399267	7999.828337	11.683341	-0.051131	4.815521
244.321334	7999.806797	11.688346	-0.051116	4.815515
244.352780	7999.874602	11.693351	-0.051122	4.815535
244.238609	7999.832182	11.698355	-0.051101	4.815523
244.154208	7999.772093	11.703360	-0.051086	4.815506
244.234373	7999.842828	11.708365	-0.051101	4.815526
244.499184	7999.913368	11.713370	-0.051150	4.815546
244.355234	7999.793576	11.718375	-0.051124	4.815511
244.432035	7999.845035	11.723379	-0.051138	4.815526
244.095890	7999.831034	11.728384	-0.051076	4.815523
244.120461	7999.834656	11.733389	-0.051081	4.815524
244.187857	7999.900911	11.738394	-0.051093	4.815543
244.403054	7999.767749	11.743399	-0.051134	4.815503
244.508985	7999.834633	11.748403	-0.051154	4.815523
244.430480	7999.871815	11.753408	-0.051139	4.815534
244.673498	7999.791432	11.758413	-0.051185	4.815509
244.566902	7999.830292	11.763418	-0.051165	4.815521
244.492722	7999.806676	11.768423	-0.051151	4.815514
244.545967	7999.843870	11.773427	-0.051162	4.815525
244.445217	7999.851857	11.778432	-0.051143	4.815528
244.442479	7999.820863	11.783437	-0.051143	4.815519
244.611451	7999.922946	11.788442	-0.051174	4.815548
244.503163	7999.846449	11.793447	-0.051154	4.815526
244.502552	7999.889172	11.798451	-0.051155	4.815538
244.620061	7999.851593	11.803456	-0.051177	4.815527
244.606920	7999.836447	11.808461	-0.051174	4.815523
244.532037	7999.864078	11.813466	-0.051161	4.815531
244.403315	7999.794723	11.818471	-0.051137	4.815511
244.562681	7999.939364	11.823475	-0.051167	4.815553
244.520008	7999.813747	11.828480	-0.051159	4.815516
244.709207	7999.855291	11.833485	-0.051194	4.815528
244.556538	7999.831464	11.838490	-0.051166	4.815521
244.479517	7999.788581	11.843495	-0.051152	4.815509
244.467709	7999.909075	11.848499	-0.051150	4.815544
244.726086	7999.811856	11.853504	-0.051198	4.815515
244.934189	7999.901764	11.858509	-0.051237	4.815540
244.775554	7999.845803	11.863514	-0.051208	4.815524
244.755385	7999.810252	11.868519	-0.051204	4.815514
244.641596	7999.875692	11.873523	-0.051184	4.815534
244.712190	7999.821332	11.878528	-0.051197	4.815518
244.785907	7999.863130	11.883533	-0.051211	4.815529
244.530808	7999.882484	11.888538	-0.051164	4.815536
244.510040	7999.801006	11.893543	-0.051160	4.815513
244.457693	7999.849293	11.898547	-0.051150	4.815527
244.547603	7999.860388	11.903552	-0.051167	4.815530
244.972245	7999.902566	11.908557	-0.051247	4.815540
244.735989	7999.830390	11.913562	-0.051203	4.815520
244.719992	7999.785297	11.918567	-0.051200	4.815507
244.829673	7999.813799	11.923571	-0.051221	4.815515
244.921630	7999.921036	11.928576	-0.051238	4.815546
244.750301	7999.794388	11.933581	-0.051206	4.815509
244.717467	7999.844061	11.938586	-0.051200	4.815524
244.706230	7999.778756	11.943591	-0.051198	4.815505
244.769637	7999.869509	11.948595	-0.051211	4.815531
244.621271	7999.858566	11.953600	-0.051183	4.815529
244.849826	7999.838816	11.958605	-0.051226	4.815522
244.809058	7999.827491	11.963610	-0.051218	4.815519
244.816362	7999.891701	11.968615	-0.051220	4.815537
244.886643	7999.859760	11.973619	-0.051233	4.815528
244.885574	7999.808503	11.978624	-0.051233	4.815513
244.918895	7999.842168	11.983629	-0.051240	4.815523
244.868158	7999.857378	11.988634	-0.051231	4.815527
244.758392	7999.851336	11.993639	-0.051210	4.815526
244.975532	7999.904015	11.998643	-0.051251	4.815540
244.709644	7999.937076	12.003648	-0.051202	4.815551
244.696525	7999.818346	12.008653	-0.051199	4.815517
244.762322	7999.832251	12.013658	-0.051212	4.815520
244.877931	7999.813863	12.018663	-0.051234	4.815514
244.973017	7999.873097	12.023667	-0.051252	4.815531
245.011506	7999.927136	12.028672	-0.051259	4.815547
245.022267	7999.804524	12.033677	-0.051261	4.815511
244.881106	7999.868450	12.038682	-0.051235	4.815530
244.672551	7999.823422	12.043687	-0.051196	4.815518
244.730568	7999.867101	12.048691	-0.051207	4.815531
244.498646	7999.911393	12.053696	-0.051164	4.815545
244.791495	7999.853180	12.058701	-0.051219	4.815526
244.796201	7999.851139	12.063706	-0.051220	4.815526
244.676551	7999.854546	12.068711	-0.051198	4.815527
244.802220	7999.828848	12.073715	-0.051222	4.815519
244.731116	7999.876830	12.078720	-0.051209	4.815533
244.821767	7999.833474	12.083725	-0.051226	4.815520
244.660314	7999.811640	12.088730	-0.051196	4.815515
244.778019	7999.853087	12.093735	-0.051218	4.815526
245.037313	7999.793259	12.098739	-0.051267	4.815508
244.768854	7999.917047	12.103744	-0.051217	4.815545
244.855875	7999.825578	12.108749	-0.051233	4.815518
244.705428	7999.840231	12.113754	-0.051205	4.815523
244.651169	7999.783835	12.118759	-0.051195	4.815507
244.675329	7999.875016	12.123763	-0.051200	4.815533
244.591198	7999.872596	12.128768	-0.051185	4.815533
244.754762	7999.828293	12.133773	-0.051215	4.815519
244.734203	7999.843994	12.138778	-0.051212	4.815524
244.736454	7999.787452	12.143783	-0.051212	4.815507
244.765247	7999.842401	12.148787	-0.051218	4.815523
244.613061	7999.882654	12.153792	-0.051190	4.815536
244.685598	7999.789881	12.158797	-0.051204	4.815508
244.817741	7999.845447	12.163802	-0.051228	4.815524
244.523605	7999.910083	12.168807	-0.051174	4.815544
244.707109	7999.872513	12.173811	-0.051208	4.815532
244.758924	7999.809303	12.178816	-0.051218	4.815513
244.897964	7999.803044	12.183821	-0.051244	4.815511
244.845846	7999.928222	12.188826	-0.051235	4.815548
244.844153	7999.823561	12.193831	-0.051235	4.815517
245.004307	7999.855022	12.198835	-0.051265	4.815526
244.553907	7999.834885	12.203840	-0.051181	4.815522
244.719728	7999.811977	12.208845	-0.051212	4.815514
244.814480	7999.846643	12.213850	-0.051230	4.815524
244.781456	7999.816223	12.218855	-0.051224	4.815515
244.856138	7999.918907	12.223859	-0.051238	4.815545
244.882995	7999.838204	12.228864	-0.051243	4.815521
245.076098	7999.857387	12.233869	-0.051279	4.815526
244.939540	7999.856248	12.238874	-0.051254	4.815526
244.960978	7999.826715	12.243879	-0.051258	4.815518
244.885295	7999.933355	12.248883	-0.051245	4.815549
244.831462	7999.859880	12.253888	-0.051235	4.815528
244.890908	7999.839510	12.258893	-0.051246	4.815522
245.114710	7999.890162	12.263898	-0.051288	4.815535
244.655792	7999.788728	12.268903	-0.051203	4.815508
244.700000	7999.833249	12.273907	-0.051211	4.815521
244.989661	7999.899925	12.278912	-0.051265	4.815539
245.039725	7999.835619	12.283917	-0.051275	4.815520
244.789009	7999.950085	12.288922	-0.051228	4.815554
244.851037	7999.761032	12.293927	-0.051240	4.815499
244.751368	7999.864078	12.298931	-0.051222	4.815529
244.597643	7999.834894	12.303936	-0.051193	4.815522
244.696958	7999.876042	12.308941	-0.051212	4.815533
244.877647	7999.886480	12.313946	-0.051246	4.815535
244.871691	7999.869315	12.318951	-0.051245	4.815530
244.831092	7999.862265	12.323955	-0.051238	4.815528
244.868327	7999.818039	12.328960	-0.051245	4.815515
245.031045	7999.850610	12.333965	-0.051275	4.815524
244.969799	7999.836815	12.338970	-0.051264	4.815520
244.981770	7999.832757	12.343975	-0.051266	4.815519
245.002740	7999.854474	12.348979	-0.051271	4.815525
244.994371	7999.920565	12.353984	-0.051269	4.815545
244.963880	7999.787669	12.358989	-0.051264	4.815506
245.046578	7999.845633	12.363994	-0.051279	4.815523
244.790326	7999.850017	12.368999	-0.051232	4.815525
244.731045	7999.911006	12.374003	-0.051221	4.815543
244.709600	7999.843399	12.379008	-0.051217	4.815523
244.761157	7999.823968	12.384013	-0.051227	4.815518
244.631867	7999.842169	12.389018	-0.051203	4.815523
244.778631	7999.814678	12.394023	-0.051231	4.815515
245.009203	7999.877187	12.399027	-0.051274	4.815532
244.929121	7999.840660	12.404032	-0.051259	4.815522
244.838568	7999.854153	12.409037	-0.051242	4.815526
244.958189	7999.954366	12.414042	-0.051265	4.815555
244.874810	7999.834490	12.419047	-0.051250	4.815520
244.885905	7999.893423	12.424051	-0.051252	4.815537
244.799851	7999.871749	12.429056	-0.051236	4.815531
244.858676	7999.894083	12.434061	-0.051247	4.815537
244.936688	7999.846250	12.439066	-0.051262	4.815523
244.944662	7999.794072	12.444071	-0.051264	4.815508
244.958185	7999.870131	12.449075	-0.051266	4.815530
245.069569	7999.936038	12.454080	-0.051287	4.815549
244.734263	7999.884671	12.459085	-0.051225	4.815535
244.815385	7999.861450	12.464090	-0.051240	4.815528
244.814803	7999.790979	12.469095	-0.051240	4.815508
244.892730	7999.834983	12.474099	-0.051255	4.815520
244.817020	7999.911722	12.479104	-0.051241	4.815543
244.928721	7999.804637	12.484109	-0.051262	4.815511
245.011555	7999.883961	12.489114	-0.051278	4.815534
244.853474	7999.916642	12.494119	-0.051249	4.815544
245.113049	7999.858954	12.499123	-0.051297	4.815526
245.075698	7999.822056	12.504128	-0.051291	4.815515
244.941681	7999.828433	12.509133	-0.051266	4.815518
245.112816	7999.873956	12.514138	-0.051298	4.815530
245.065305	7999.843299	12.519143	-0.051289	4.815522
244.834737	7999.874799	12.524147	-0.051247	4.815532
245.045702	7999.850491	12.529152	-0.051286	4.815524
245.134186	7999.857291	12.534157	-0.051303	4.815525
245.001120	7999.981150	12.539162	-0.051278	4.815562
244.925783	7999.831505	12.544167	-0.051264	4.815519
244.975665	7999.886798	12.549171	-0.051274	4.815535
245.164980	7999.850390	12.554176	-0.051309	4.815523
244.994991	7999.857248	12.559181	-0.051278	4.815526
244.961903	7999.919733	12.564186	-0.051272	4.815544
245.033531	7999.862185	12.569191	-0.051285	4.815527
245.112722	7999.859222	12.574195	-0.051300	4.815526
244.886926	7999.904683	12.579200	-0.051259	4.815540
244.915681	7999.820807	12.584205	-0.051264	4.815516
245.270988	7999.874671	12.589210	-0.051330	4.815530
245.117005	7999.956543	12.594215	-0.051302	4.815554
244.844769	7999.886982	12.599219	-0.051252	4.815535
245.074506	7999.873659	12.604224	-0.051295	4.815530
244.933401	7999.809440	12.609229	-0.051268	4.815512
244.969080	7999.828194	12.614234	-0.051275	4.815518
245.069955	7999.857621	12.619239	-0.051294	4.815526
244.997676	7999.792388	12.624243	-0.051281	4.815507
244.983944	7999.908582	12.629248	-0.051279	4.815541
245.024809	7999.837718	12.634253	-0.051286	4.815520
244.943811	7999.875927	12.639258	-0.051272	4.815532
244.939651	7999.824619	12.644263	-0.051271	4.815517
244.911286	7999.952321	12.649267	-0.051266	4.815554
244.899926	7999.832552	12.654272	-0.051264	4.815519
244.726730	7999.872462	12.659277	-0.051232	4.815532
244.741159	7999.854562	12.664282	-0.051235	4.815526
244.850701	7999.795496	12.669287	-0.051256	4.815508
244.955625	7999.835668	12.674291	-0.051275	4.815520
244.825153	7999.907243	12.679296	-0.051251	4.815541
244.999812	7999.776623	12.684301	-0.051284	4.815502
244.978143	7999.945014	12.689306	-0.051280	4.815552
244.919669	7999.775353	12.694311	-0.051269	4.815502
245.185158	7999.824550	12.699315	-0.051319	4.815515
245.063734	7999.930445	12.704320	-0.051297	4.815547
244.892289	7999.829424	12.709325	-0.051265	4.815518
244.907785	7999.880953	12.714330	-0.051268	4.815533
244.915590	7999.861876	12.719335	-0.051270	4.815528
244.868849	7999.872879	12.724339	-0.051261	4.815531
244.991996	7999.909077	12.729344	-0.051284	4.815541
244.948488	7999.804801	12.734349	-0.051276	4.815511
245.245447	7999.859851	12.739354	-0.051332	4.815525
245.017218	7999.851877	12.744359	-0.051290	4.815524
244.955759	7999.906423	12.749363	-0.051278	4.815540
244.973582	7999.824505	12.754368	-0.051282	4.815516
244.988902	7999.799144	12.759373	-0.051285	4.815509
244.942061	7999.981007	12.764378	-0.051277	4.815562
245.043796	7999.824636	12.769383	-0.051296	4.815516
245.083910	7999.863752	12.774387	-0.051303	4.815527
245.118050	7999.828019	12.779392	-0.051310	4.815517
245.068619	7999.934020	12.784397	-0.051301	4.815548
245.176129	7999.931519	12.789402	-0.051321	4.815547
245.103641	7999.911134	12.794407	-0.051308	4.815541
245.000218	7999.866751	12.799411	-0.051289	4.815528
244.982533	7999.839783	12.804416	-0.051286	4.815521
245.001607	7999.887099	12.809421	-0.051289	4.815534
245.077640	7999.880882	12.814426	-0.051304	4.815532
245.154492	7999.880017	12.819431	-0.051318	4.815532
245.243189	7999.885753	12.824435	-0.051335	4.815533
245.144306	7999.899109	12.829440	-0.051317	4.815537
245.059367	7999.843281	12.834445	-0.051301	4.815521
245.201404	7999.863768	12.839450	-0.051328	4.815527
244.793219	7999.848590	12.844455	-0.051252	4.815524
244.795796	7999.871076	12.849459	-0.051253	4.815531
244.952092	7999.927036	12.854464	-0.051282	4.815546
244.912873	7999.824966	12.859469	-0.051275	4.815517
244.905829	7999.849430	12.864474	-0.051274	4.815524
244.752807	7999.791425	12.869479	-0.051246	4.815508
245.085319	7999.816084	12.874483	-0.051308	4.815513
244.890293	7999.969903	12.879488	-0.051272	4.815559
244.997912	7999.869158	12.884493	-0.051292	4.815529
245.151772	7999.872752	12.889498	-0.051321	4.815529
244.973934	7999.794052	12.894503	-0.051288	4.815507
244.916974	7999.850807	12.899507	-0.051277	4.815524
244.791486	7999.912853	12.904512	-0.051254	4.815543
244.979536	7999.818759	12.909517	-0.051289	4.815514
245.015121	7999.871684	12.914522	-0.051296	4.815530
244.796323	7999.856389	12.919527	-0.051256	4.815526
245.025331	7999.819560	12.924531	-0.051299	4.815514
245.112591	7999.831679	12.929536	-0.051315	4.815518
244.942052	7999.831054	12.934541	-0.051284	4.815518
244.996573	7999.877880	12.939546	-0.051294	4.815532
244.855479	7999.915110	12.944551	-0.051268	4.815543
245.135776	7999.842809	12.949555	-0.051320	4.815521
245.020235	7999.832401	12.954560	-0.051299	4.815518
245.044844	7999.847771	12.959565	-0.051304	4.815523
244.805171	7999.853493	12.964570	-0.051259	4.815525
245.006549	7999.873880	12.969575	-0.051297	4.815530
245.120796	7999.982550	12.974579	-0.051319	4.815562
244.913120	7999.843561	12.979584	-0.051280	4.815522
245.119748	7999.838404	12.984589	-0.051319	4.815519
245.103691	7999.885147	12.989594	-0.051316	4.815533
245.071325	7999.831243	12.994599	-0.051310	4.815518
245.242726	7999.890654	12.999603	-0.051342	4.815534
245.164359	7999.970555	13.004608	-0.051328	4.815558
244.999399	7999.872841	13.009613	-0.051297	4.815530
245.214204	7999.874225	13.014618	-0.051338	4.815529
244.923032	7999.863090	13.019623	-0.051284	4.815528
245.227389	7999.900106	13.024627	-0.051340	4.815537
245.049443	7999.829946	13.029632	-0.051308	4.815517
245.234306	7999.868218	13.034637	-0.051342	4.815528
245.241239	7999.896115	13.039642	-0.051344	4.815536
245.193477	7999.944477	13.044647	-0.051335	4.815550
245.008323	7999.845367	13.049651	-0.051301	4.815522
245.173190	7999.892924	13.054656	-0.051332	4.815535
245.091199	7999.885199	13.059661	-0.051317	4.815533
245.216153	7999.891525	13.064666	-0.051340	4.815534
245.185879	7999.861149	13.069671	-0.051335	4.815526
245.284030	7999.875582	13.074675	-0.051353	4.815529
245.094396	7999.851151	13.079680	-0.051318	4.815523
245.187312	7999.939183	13.084685	-0.051336	4.815548
245.250126	7999.937022	13.089690	-0.051347	4.815547
245.255764	7999.863447	13.094695	-0.051349	4.815526
245.204346	7999.833794	13.099699	-0.051339	4.815518
245.049083	7999.877201	13.104704	-0.051311	4.815531
245.173464	7999.837599	13.109709	-0.051334	4.815519
245.141720	7999.912920	13.114714	-0.051328	4.815541
245.078333	7999.904429	13.119719	-0.051317	4.815539
245.062317	7999.834774	13.124723	-0.051314	4.815518
245.119350	7999.852808	13.129728	-0.051325	4.815523
245.035223	7999.819418	13.134733	-0.051309	4.815514
245.046299	7999.898640	13.139738	-0.051312	4.815537
245.106711	7999.834502	13.144743	-0.051323	4.815518
245.241035	7999.805741	13.149747	-0.051348	4.815509
244.966821	7999.957201	13.154752	-0.051297	4.815555
245.075966	7999.846870	13.159757	-0.051318	4.815522
245.236555	7999.889018	13.164762	-0.051348	4.815533
245.006227	7999.822276	13.169767	-0.051305	4.815515
245.122289	7999.898939	13.174771	-0.051327	4.815537
245.202457	7999.908807	13.179776	-0.051342	4.815539
245.086796	7999.812965	13.184781	-0.051321	4.815512
245.129297	7999.873478	13.189786	-0.051329	4.815529
244.923377	7999.816746	13.194791	-0.051291	4.815514
244.956601	7999.960402	13.199795	-0.051297	4.815556
245.020205	7999.837582	13.204800	-0.051309	4.815519
245.064611	7999.840460	13.209805	-0.051318	4.815520
244.993066	7999.887367	13.214810	-0.051305	4.815534
244.917430	7999.920325	13.219815	-0.051291	4.815544
245.090829	7999.835602	13.224819	-0.051323	4.815518
245.111261	7999.854108	13.229824	-0.051327	4.815524
245.135095	7999.828885	13.234829	-0.051332	4.815516
245.091475	7999.861297	13.239834	-0.051324	4.815526
245.063046	7999.835222	13.244839	-0.051319	4.815518
245.267841	7999.957115	13.249843	-0.051357	4.815553
245.069102	7999.832154	13.254848	-0.051321	4.815518
245.147923	7999.837728	13.259853	-0.051335	4.815519
245.190870	7999.965526	13.264858	-0.051344	4.815556
245.191938	7999.857704	13.269863	-0.051344	4.815524
245.072090	7999.880330	13.274867	-0.051322	4.815532
245.060442	7999.865208	13.279872	-0.051320	4.815527
245.069093	7999.844010	13.284877	-0.051322	4.815521
245.067388	7999.869629	13.289882	-0.051322	4.815528
245.134196	7999.871805	13.294887	-0.051334	4.815529
245.107253	7999.922642	13.299891	-0.051330	4.815544
245.071171	7999.897511	13.304896	-0.051323	4.815537
245.192442	7999.870673	13.309901	-0.051346	4.815528
245.241122	7999.902454	13.314906	-0.051355	4.815537
244.997269	7999.934805	13.319911	-0.051310	4.815548
245.261069	7999.912426	13.324915	-0.051359	4.815540
245.184700	7999.885570	13.329920	-0.051345	4.815532
245.136923	7999.855976	13.334925	-0.051336	4.815524
245.223064	7999.888368	13.339930	-0.051353	4.815533
245.331517	7999.855981	13.344935	-0.051373	4.815523
245.270054	7999.874220	13.349939	-0.051362	4.815529
245.031179	7999.884226	13.354944	-0.051318	4.815533
245.006938	7999.881714	13.359949	-0.051313	4.815532
245.204086	7999.927662	13.364954	-0.051350	4.815545
245.118623	7999.924151	13.369959	-0.051335	4.815544
244.984591	7999.867521	13.374963	-0.051310	4.815528
245.018593	7999.901198	13.379968	-0.051316	4.815538
244.958020	7999.867125	13.384973	-0.051305	4.815528
245.136041	7999.906353	13.389978	-0.051339	4.815539
245.192741	7999.869919	13.394983	-0.051349	4.815528
245.252891	7999.902955	13.399987	-0.051361	4.815537
245.117961	7999.908249	13.404992	-0.051336	4.815539
245.131963	7999.855101	13.409997	-0.051339	4.815524
245.297769	7999.896266	13.415002	-0.051370	4.815535
245.019725	7999.831950	13.420007	-0.051318	4.815518
245.011756	7999.880961	13.425011	-0.051317	4.815532
245.154412	7999.979415	13.430016	-0.051344	4.815560
245.285757	7999.881193	13.435021	-0.051368	4.815531
245.185145	7999.924422	13.440026	-0.051350	4.815544
245.003284	7999.887303	13.445031	-0.051316	4.815534
245.128474	7999.901109	13.450035	-0.051340	4.815537
245.257484	7999.893619	13.455040	-0.051364	4.815534
245.055849	7999.899961	13.460045	-0.051327	4.815537
245.211629	7999.908927	13.465050	-0.051356	4.815539
245.173207	7999.781239	13.470055	-0.051349	4.815502
245.151893	7999.885563	13.475059	-0.051345	4.815532
245.387682	7999.909716	13.480064	-0.051389	4.815538
245.212120	7999.832119	13.485069	-0.051357	4.815517
245.151346	7999.960362	13.490074	-0.051346	4.815554
245.173769	7999.896672	13.495079	-0.051350	4.815536
245.319500	7999.902269	13.500083	-0.051377	4.815537
245.379804	7999.884049	13.505088	-0.051389	4.815531
245.255101	7999.863880	13.510093	-0.051366	4.815526
245.115748	7999.890459	13.515098	-0.051340	4.815534
245.236371	7999.861475	13.520103	-0.051363	4.815525
245.260976	7999.885388	13.525107	-0.051368	4.815532
245.325217	7999.902472	13.530112	-0.051380	4.815537
245.288974	7999.938208	13.535117	-0.051373	4.815547
245.101361	7999.897791	13.540122	-0.051338	4.815536
245.074276	7999.862127	13.545127	-0.051334	4.815526
245.435353	7999.913952	13.550131	-0.051401	4.815539
245.394088	7999.902618	13.555136	-0.051394	4.815536
245.229989	7999.910640	13.560141	-0.051363	4.815539
245.196703	7999.940016	13.565146	-0.051357	4.815548
245.339736	7999.863342	13.570151	-0.051384	4.815525
245.100635	7999.847716	13.575155	-0.051340	4.815522
245.359433	7999.929909	13.580160	-0.051388	4.815544
245.351942	7999.842238	13.585165	-0.051387	4.815519
245.338809	7999.937085	13.590170	-0.051385	4.815547
245.121493	7999.880165	13.595175	-0.051344	4.815531
245.142857	7999.894414	13.600179	-0.051349	4.815535
245.132388	7999.909212	13.605184	-0.051347	4.815539
245.014530	7999.864594	13.610189	-0.051325	4.815527
245.066080	7999.877199	13.615194	-0.051335	4.815530
245.023951	7999.940604	13.620199	-0.051327	4.815549
245.054869	7999.867441	13.625203	-0.051333	4.815528
244.959054	7999.879780	13.630208	-0.051316	4.815532
245.145387	7999.894583	13.635213	-0.051351	4.815535
245.296223	7999.908807	13.640218	-0.051379	4.815538
245.210786	7999.852970	13.645223	-0.051363	4.815523
245.241562	7999.917564	13.650227	-0.051369	4.815541
245.220311	7999.891606	13.655232	-0.051365	4.815534
245.346908	7999.885145	13.660237	-0.051389	4.815531
245.326372	7999.946766	13.665242	-0.051386	4.815549
245.362832	7999.906799	13.670247	-0.051393	4.815537
245.209848	7999.890440	13.675251	-0.051364	4.815533
245.117937	7999.895367	13.680256	-0.051347	4.815535
245.320093	7999.902953	13.685261	-0.051385	4.815537
245.289048	7999.980422	13.690266	-0.051380	4.815559
245.271004	7999.861609	13.695271	-0.051376	4.815525
245.247968	7999.859116	13.700275	-0.051372	4.815524
245.422172	7999.903622	13.705280	-0.051405	4.815536
245.058932	7999.883836	13.710285	-0.051338	4.815532
245.460562	7999.913896	13.715290	-0.051413	4.815539
245.457406	7999.927745	13.720295	-0.051412	4.815543
245.562760	7999.904919	13.725299	-0.051432	4.815536
245.444027	7999.915816	13.730304	-0.051410	4.815540
245.377987	7999.916894	13.735309	-0.051398	4.815540
245.568174	7999.915741	13.740314	-0.051434	4.815539
245.285284	7999.873771	13.745319	-0.051381	4.815528
245.303235	7999.845248	13.750323	-0.051385	4.815520
245.344292	7999.944183	13.755328	-0.051393	4.815548
245.323890	7999.847757	13.760333	-0.051389	4.815520
245.529391	7999.894910	13.765338	-0.051427	4.815533
245.491243	7999.868676	13.770343	-0.051421	4.815526
245.367724	7999.929687	13.775347	-0.051398	4.815544
245.198289	7999.898109	13.780352	-0.051366	4.815536
245.237155	7999.866724	13.785357	-0.051374	4.815526
245.301808	7999.953229	13.790362	-0.051386	4.815551
245.320103	7999.946070	13.795367	-0.051390	4.815549
245.181752	7999.918203	13.800371	-0.051364	4.815542
245.294341	7999.961705	13.805376	-0.051385	4.815554
245.077687	7999.835382	13.810381	-0.051345	4.815518
245.046964	7999.873344	13.815386	-0.051340	4.815529
245.281338	7999.860097	13.820391	-0.051384	4.815524
245.500013	7999.871155	13.825395	-0.051424	4.815526
245.434875	7999.921371	13.830400	-0.051413	4.815541
245.395945	7999.909007	13.835405	-0.051406	4.815538
245.506101	7999.928976	13.840410	-0.051426	4.815543
245.282457	7999.928552	13.845415	-0.051385	4.815544
245.162085	7999.876416	13.850419	-0.051363	4.815529
245.333530	7999.885637	13.855424	-0.051395	4.815531
245.198873	7999.932583	13.860429	-0.051370	4.815546
245.178861	7999.889559	13.865434	-0.051366	4.815533
245.256353	7999.885501	13.870439	-0.051381	4.815532
245.461260	7999.848280	13.875443	-0.051419	4.815520
245.220771	7999.892433	13.880448	-0.051375	4.815534
245.314977	7999.888647	13.885453	-0.051393	4.815532
245.494218	7999.923625	13.890458	-0.051426	4.815542
245.493666	7999.874511	13.895463	-0.051426	4.815527
245.517822	7999.906960	13.900467	-0.051431	4.815537
245.734592	7999.923328	13.905472	-0.051472	4.815540
245.457079	7999.849407	13.910477	-0.051420	4.815520
245.194481	8000.005329	13.915482	-0.051371	4.815567
245.114781	7999.897258	13.920487	-0.051357	4.815536
245.441521	7999.909010	13.925491	-0.051418	4.815537
245.360598	7999.888487	13.930496	-0.051403	4.815532
245.208273	7999.900972	13.935501	-0.051375	4.815536
245.408131	7999.921336	13.940506	-0.051412	4.815541
245.183413	7999.905943	13.945511	-0.051371	4.815538
245.007713	7999.890282	13.950515	-0.051338	4.815534
245.182762	7999.902765	13.955520	-0.051371	4.815537
245.214747	7999.876607	13.960525	-0.051377	4.815529
245.366975	7999.882311	13.965530	-0.051406	4.815530
245.314778	7999.828083	13.970535	-0.051396	4.815514
245.429013	7999.872680	13.975539	-0.051418	4.815527
245.230728	7999.895095	13.980544	-0.051381	4.815534
245.160261	7999.948427	13.985549	-0.051368	4.815550
245.447107	7999.943511	13.990554	-0.051422	4.815547
245.427230	7999.906897	13.995559	-0.051418	4.815537
245.572807	7999.896474	14.000563	-0.051445	4.815533
245.509144	7999.929627	14.005568	-0.051434	4.815543
245.614925	7999.867295	14.010573	-0.051454	4.815524
245.630099	7999.876104	14.015578	-0.051457	4.815527
245.490225	7999.864231	14.020583	-0.051431	4.815524
245.647951	7999.908469	14.025587	-0.051460	4.815536
245.533622	7999.910895	14.030592	-0.051439	4.815537
245.418232	7999.969902	14.035597	-0.051418	4.815555
245.398002	7999.899109	14.040602	-0.051414	4.815535
245.399815	7999.817996	14.045607	-0.051415	4.815511
245.425075	7999.894247	14.050611	-0.051420	4.815533
245.464627	7999.951509	14.055616	-0.051428	4.815550
245.554720	7999.902805	14.060621	-0.051444	4.815535
245.346880	7999.900502	14.065626	-0.051406	4.815535
245.419377	7999.901702	14.070631	-0.051420	4.815535
245.334725	7999.823451	14.075635	-0.051404	4.815513
245.297008	7999.965953	14.080640	-0.051397	4.815555
245.215549	7999.888822	14.085645	-0.051382	4.815532
245.389289	7999.908760	14.090650	-0.051415	4.815537
245.420697	7999.919969	14.095655	-0.051421	4.815541
245.345893	7999.947601	14.100659	-0.051407	4.815549
245.470899	7999.938979	14.105664	-0.051431	4.815546
245.493651	7999.885972	14.110669	-0.051435	4.815530
245.470001	7999.961426	14.115674	-0.051431	4.815552
245.371293	7999.932070	14.120679	-0.051413	4.815544
245.413832	7999.922102	14.125683	-0.051421	4.815541
245.242948	7999.870211	14.130688	-0.051389	4.815527
245.310564	7999.836091	14.135693	-0.051402	4.815517
245.475262	7999.886850	14.140698	-0.051433	4.815531
245.400596	7999.942250	14.145703	-0.051419	4.815547
245.130392	7999.846023	14.150707	-0.051369	4.815520
245.316639	7999.877911	14.155712	-0.051404	4.815529
245.352374	7999.828320	14.160717	-0.051411	4.815514
245.289126	7999.870023	14.165722	-0.051399	4.815527
245.256001	8000.002989	14.170727	-0.051393	4.815566
245.377675	7999.913152	14.175731	-0.051416	4.815539
245.393437	7999.926242	14.180736	-0.051419	4.815542
245.124019	7999.807602	14.185741	-0.051369	4.815509
245.425435	7999.884084	14.190746	-0.051426	4.815530
245.361386	7999.862767	14.195751	-0.051414	4.815524
245.179979	7999.935649	14.200755	-0.051381	4.815546
245.093363	7999.909693	14.205760	-0.051365	4.815539
245.283992	7999.849813	14.210765	-0.051400	4.815521
245.332376	7999.868775	14.215770	-0.051409	4.815526
245.250146	7999.847162	14.220775	-0.051394	4.815520
245.248090	7999.831128	14.225779	-0.051394	4.815515
245.314610	7999.870675	14.230784	-0.051407	4.815527
245.213241	7999.912825	14.235789	-0.051388	4.815539
245.302227	7999.896140	14.240794	-0.051405	4.815534
245.425275	7999.847973	14.245799	-0.051428	4.815519
245.448973	7999.599558	14.250803	-0.051432	4.815447

245.343782	7996.392385	14.255808	-0.051411	4.814509
245.346838	7990.768899	14.260813	-0.051408	4.812865
245.413500	7984.001425	14.265818	-0.051416	4.810884
245.243588	7976.658200	14.270823	-0.051380	4.808736
245.425351	7969.063716	14.275827	-0.051409	4.806511
245.520177	7961.225247	14.280832	-0.051422	4.804214
245.288573	7953.371699	14.285837	-0.051374	4.801913
245.371125	7945.372388	14.290842	-0.051384	4.799567
245.142340	7937.461721	14.295847	-0.051337	4.797247
245.140873	7929.417938	14.300851	-0.051331	4.794886
245.100867	7921.374382	14.305856	-0.051319	4.792524
245.160011	7913.371279	14.310861	-0.051325	4.790172
245.199836	7905.438710	14.315866	-0.051327	4.787840
245.169450	7897.356214	14.320871	-0.051317	4.785463
245.082810	7889.432908	14.325875	-0.051296	4.783132
245.071616	7881.443489	14.330880	-0.051289	4.780780
244.707843	7873.432151	14.335885	-0.051216	4.778421
244.845708	7865.430402	14.340890	-0.051236	4.776063
244.769579	7857.348300	14.345895	-0.051217	4.773680
244.618116	7849.307407	14.350899	-0.051184	4.771308
244.513065	7841.397002	14.355904	-0.051159	4.768974
244.579316	7833.407004	14.360909	-0.051167	4.766614
244.585910	7825.365286	14.365914	-0.051163	4.764239
244.321628	7817.446857	14.370919	-0.051109	4.761899
244.231552	7809.322325	14.375923	-0.051087	4.759497
244.336979	7801.419383	14.380928	-0.051102	4.757158
244.410750	7793.376543	14.385933	-0.051110	4.754777
244.230832	7785.359131	14.390938	-0.051072	4.752403
244.108869	7777.317996	14.395943	-0.051044	4.750020
244.082707	7769.293558	14.400947	-0.051034	4.747641
244.332884	7761.344467	14.405952	-0.051076	4.745283
244.139443	7753.321034	14.410957	-0.051035	4.742902
244.449587	7745.357277	14.415962	-0.051088	4.740537
244.372536	7737.366215	14.420967	-0.051068	4.738163
244.081236	7729.315146	14.425971	-0.051009	4.735771
244.341528	7721.350160	14.430976	-0.051052	4.733402
244.042132	7713.276822	14.435981	-0.050992	4.731001
244.039324	7705.294310	14.440986	-0.050986	4.728624
244.063511	7697.323398	14.445991	-0.050986	4.726250
244.115799	7689.310647	14.450995	-0.050990	4.723863
243.918186	7681.348995	14.456000	-0.050949	4.721490
243.898645	7673.296655	14.461005	-0.050940	4.719088
243.874900	7665.360305	14.466010	-0.050931	4.716720
243.625028	7657.314293	14.471015	-0.050879	4.714318
243.600825	7649.306639	14.476019	-0.050869	4.711926
243.843359	7641.258109	14.481024	-0.050910	4.709520
243.896613	7633.298834	14.486029	-0.050914	4.707139
243.688475	7625.305168	14.491034	-0.050871	4.704748
243.691519	7617.342165	14.496039	-0.050866	4.702365
243.718063	7609.304163	14.501043	-0.050866	4.699957
243.545944	7601.356453	14.506048	-0.050829	4.697576
243.291660	7593.306123	14.511053	-0.050777	4.695163
243.594397	7585.310354	14.516058	-0.050828	4.692764
243.467807	7577.258757	14.521063	-0.050800	4.690348
243.440921	7569.261847	14.526067	-0.050790	4.687947
243.376503	7561.291696	14.531072	-0.050773	4.685553
243.279337	7553.314049	14.536077	-0.050750	4.683155
243.320855	7545.294564	14.541082	-0.050752	4.680743
243.380849	7537.273074	14.546087	-0.050758	4.678330
243.397853	7529.318743	14.551091	-0.050757	4.675935
243.168730	7521.280279	14.556096	-0.050709	4.673514
242.986777	7513.110611	14.561101	-0.050670	4.671052
243.078285	7505.194955	14.566106	-0.050682	4.668666
242.989261	7497.233945	14.571111	-0.050660	4.666264
243.194614	7489.224462	14.576115	-0.050694	4.663847
243.166323	7481.277099	14.581120	-0.050683	4.661447
242.931465	7473.215346	14.586125	-0.050635	4.659011
243.015278	7465.320050	14.591130	-0.050645	4.656624
242.994377	7457.184899	14.596135	-0.050636	4.654164
243.121048	7449.222628	14.601139	-0.050655	4.651754
242.812786	7441.227151	14.606144	-0.050593	4.649334
242.902269	7433.246267	14.611149	-0.050604	4.646916
242.818616	7425.210396	14.616154	-0.050584	4.644481
242.728382	7417.273459	14.621159	-0.050562	4.642074
242.730762	7409.208160	14.626163	-0.050557	4.639627
242.750534	7401.301384	14.631168	-0.050556	4.637227
242.402824	7393.214156	14.636173	-0.050486	4.634771
242.351024	7385.171837	14.641178	-0.050471	4.632327
242.426181	7377.152424	14.646183	-0.050480	4.629889
242.492439	7369.152596	14.651187	-0.050488	4.627455
242.576436	7361.189789	14.656192	-0.050498	4.625031
242.510370	7353.189012	14.661197	-0.050481	4.622595
242.456777	7345.209907	14.666202	-0.050466	4.620164
242.569274	7337.233026	14.671207	-0.050482	4.617732
242.343158	7329.188656	14.676211	-0.050435	4.615278
242.180517	7321.175243	14.681216	-0.050400	4.612833
242.248022	7313.103723	14.686221	-0.050407	4.610369
242.042944	7305.193978	14.691226	-0.050364	4.607952
242.007967	7297.165813	14.696231	-0.050353	4.605498
241.963536	7289.188903	14.701235	-0.050339	4.603059
242.070885	7281.155900	14.706240	-0.050354	4.600601
241.949762	7273.219204	14.711245	-0.050327	4.598171
241.894158	7265.185786	14.716250	-0.050311	4.595710
242.061770	7257.113553	14.721255	-0.050337	4.593236
241.838843	7249.086038	14.726259	-0.050291	4.590775
241.877963	7241.152923	14.731264	-0.050293	4.588341
241.821587	7233.108315	14.736269	-0.050278	4.585871
242.006982	7225.149791	14.741274	-0.050307	4.583427
241.636877	7217.173555	14.746279	-0.050233	4.580975
241.818921	7209.132162	14.751283	-0.050262	4.578503
241.780144	7201.156593	14.756288	-0.050250	4.576050
241.519176	7193.122157	14.761293	-0.050196	4.573576
241.716918	7185.108852	14.766298	-0.050228	4.571109
241.718652	7177.108616	14.771303	-0.050224	4.568644
241.626401	7169.119137	14.776307	-0.050201	4.566180
241.561391	7161.130869	14.781312	-0.050184	4.563716
241.534276	7153.124541	14.786317	-0.050174	4.561245
241.377915	7145.128191	14.791322	-0.050140	4.558776
241.215535	7137.189810	14.796327	-0.050105	4.556323
241.415498	7129.118756	14.801331	-0.050137	4.553828
241.411790	7121.123701	14.806336	-0.050131	4.551355
241.236939	7113.058244	14.811341	-0.050094	4.548859
241.116324	7105.103846	14.816346	-0.050066	4.546395
241.407337	7097.066907	14.821351	-0.050115	4.543906
241.277718	7089.117231	14.826355	-0.050086	4.541441
241.381530	7081.114189	14.831360	-0.050101	4.538959
241.207382	7073.147368	14.836365	-0.050063	4.536487
241.379117	7065.169714	14.841370	-0.050090	4.534010
240.874661	7057.120390	14.846375	-0.049991	4.531508
241.024272	7049.056267	14.851379	-0.050014	4.529002
241.023975	7041.127051	14.856384	-0.050009	4.526536
240.794924	7033.090448	14.861389	-0.049961	4.524035
240.763150	7025.150176	14.866394	-0.049951	4.521562
240.725949	7017.121131	14.871399	-0.049939	4.519061
240.686653	7009.166664	14.876403	-0.049926	4.516581
240.590214	7001.130972	14.881408	-0.049903	4.514075
240.712273	6992.997004	14.886413	-0.049921	4.511537
240.808485	6985.024732	14.891418	-0.049934	4.509048
240.487661	6977.055362	14.896423	-0.049869	4.506558
240.515028	6969.059560	14.901427	-0.049869	4.504059
240.540223	6961.115118	14.906432	-0.049869	4.501574
240.426367	6953.070588	14.911437	-0.049843	4.499057
240.445270	6945.105151	14.916442	-0.049841	4.496563
240.374868	6937.063276	14.921447	-0.049823	4.494043
240.223404	6929.037680	14.926451	-0.049790	4.491527
240.205474	6921.049174	14.931456	-0.049782	4.489022
240.252319	6913.049576	14.936461	-0.049785	4.486512
240.332256	6905.064048	14.941466	-0.049795	4.484005
240.000242	6897.118040	14.946471	-0.049728	4.481508
240.093270	6889.045003	14.951475	-0.049741	4.478970
240.060590	6881.108863	14.956480	-0.049730	4.476474
240.021923	6873.057223	14.961485	-0.049717	4.473940
239.981385	6865.031005	14.966490	-0.049705	4.471413
240.079371	6857.015700	14.971495	-0.049718	4.468888
240.001895	6849.003951	14.976499	-0.049699	4.466363
239.960536	6841.010203	14.981504	-0.049686	4.463841
239.854091	6833.041552	14.986509	-0.049661	4.461326
239.967537	6825.062916	14.991514	-0.049677	4.458807
239.721293	6817.050704	14.996519	-0.049626	4.456275
239.732292	6809.023146	15.001523	-0.049623	4.453738
239.785966	6801.003571	15.006528	-0.049628	4.451201
239.602619	6792.977806	15.011533	-0.049589	4.448661
239.546656	6785.017133	15.016538	-0.049574	4.446140
239.601558	6776.998455	15.021543	-0.049579	4.443599
239.669480	6769.017648	15.026547	-0.049587	4.441069
239.657868	6761.027697	15.031552	-0.049579	4.438535
239.628137	6753.042574	15.036557	-0.049569	4.436001
239.481838	6744.986030	15.041562	-0.049537	4.433441
239.300206	6736.986767	15.046567	-0.049498	4.430899
239.296468	6728.963098	15.051571	-0.049492	4.428348
239.195897	6720.992574	15.056576	-0.049468	4.425812
239.140051	6712.938733	15.061581	-0.049453	4.423248
239.372277	6704.991098	15.066586	-0.049491	4.420718
239.178272	6697.001531	15.071591	-0.049450	4.418171
239.268118	6688.969208	15.076595	-0.049462	4.415610
239.309534	6680.963795	15.081600	-0.049464	4.413057
239.009425	6672.974274	15.086605	-0.049404	4.410505
239.040164	6664.988117	15.091610	-0.049404	4.407954
239.046932	6656.986457	15.096615	-0.049401	4.405397
238.614842	6648.987859	15.101619	-0.049315	4.402837
238.863875	6641.028641	15.106624	-0.049357	4.400291
238.784007	6633.026812	15.111629	-0.049337	4.397729
238.727183	6625.012732	15.116634	-0.049321	4.395162
238.657525	6616.975347	15.121639	-0.049303	4.392585
238.707180	6608.928964	15.126643	-0.049307	4.390005
238.765323	6600.964958	15.131648	-0.049313	4.387449
238.741741	6592.959397	15.136653	-0.049304	4.384879
238.512523	6585.007896	15.141658	-0.049256	4.382323
238.556840	6576.974618	15.146663	-0.049259	4.379741
238.482499	6569.032659	15.151667	-0.049240	4.377185
238.636622	6561.019383	15.156672	-0.049264	4.374607
238.337363	6552.959174	15.161677	-0.049203	4.372010
238.255596	6544.930764	15.166682	-0.049183	4.369422
238.265708	6536.977027	15.171687	-0.049180	4.366858
238.494911	6528.964725	15.176691	-0.049218	4.364274
238.637965	6521.052548	15.181696	-0.049239	4.361721
238.271417	6512.973322	15.186701	-0.049166	4.359109
238.426414	6505.017165	15.191706	-0.049190	4.356539
238.479907	6496.981789	15.196711	-0.049195	4.353941
238.008723	6488.887557	15.201715	-0.049102	4.351319
238.326095	6480.909512	15.206720	-0.049156	4.348738
238.143969	6472.924242	15.211725	-0.049117	4.346150
238.076974	6464.994364	15.216730	-0.049100	4.343579
238.083802	6456.953154	15.221735	-0.049096	4.340971
237.909117	6448.960064	15.226739	-0.049059	4.338375
237.938391	6441.003024	15.231744	-0.049059	4.335791
237.656482	6432.933546	15.236749	-0.049001	4.333167
237.790597	6424.932955	15.241754	-0.049021	4.330567
237.919364	6416.970818	15.246759	-0.049040	4.327978
237.768683	6408.923729	15.251763	-0.049007	4.325357
237.747306	6400.954386	15.256768	-0.048998	4.322761
237.491563	6392.961624	15.261773	-0.048946	4.320154
237.757676	6385.025072	15.266778	-0.048990	4.317568
237.620093	6376.940809	15.271783	-0.048960	4.314929
237.589535	6368.900178	15.276787	-0.048949	4.312303
237.652263	6360.898585	15.281792	-0.048956	4.309690
237.475944	6352.945648	15.286797	-0.048918	4.307088
237.467686	6344.933493	15.291802	-0.048911	4.304467
237.494320	6336.959720	15.296807	-0.048911	4.301858
237.322253	6328.922200	15.301811	-0.048874	4.299224
237.558233	6320.987374	15.306816	-0.048913	4.296626
237.204178	6312.924200	15.311821	-0.048842	4.293979
237.240039	6304.904071	15.316826	-0.048844	4.291348
237.121892	6296.895543	15.321831	-0.048817	4.288717
236.935182	6288.909854	15.326835	-0.048777	4.286092
237.115027	6280.942654	15.331840	-0.048806	4.283475
236.873851	6272.964423	15.336845	-0.048756	4.280849
236.714061	6264.982464	15.341850	-0.048721	4.278220
236.902010	6256.952888	15.346855	-0.048751	4.275577
236.783603	6248.876529	15.351859	-0.048724	4.272915
236.843118	6240.917007	15.356864	-0.048730	4.270291
236.693872	6232.894102	15.361869	-0.048697	4.267643
236.681530	6224.843291	15.366874	-0.048690	4.264984
236.729636	6216.910203	15.371879	-0.048694	4.262364
236.580315	6208.856080	15.376883	-0.048661	4.259700
236.662473	6200.924367	15.381888	-0.048671	4.257078
236.469467	6192.866444	15.386893	-0.048630	4.254409
236.504215	6184.895014	15.391898	-0.048632	4.251769
236.515764	6176.904686	15.396903	-0.048629	4.249122
236.293987	6168.900464	15.401907	-0.048583	4.246465
236.474184	6160.892831	15.406912	-0.048611	4.243810
236.322508	6152.935291	15.411917	-0.048578	4.241167
236.276600	6144.975998	15.416922	-0.048564	4.238522
236.156603	6136.987216	15.421927	-0.048537	4.235865
236.128704	6128.935154	15.426931	-0.048527	4.233187
236.381302	6120.915658	15.431936	-0.048569	4.230520
236.192005	6112.890671	15.436941	-0.048529	4.227845
236.219769	6104.908446	15.441946	-0.048529	4.225185
236.276805	6096.923822	15.446951	-0.048534	4.222523
235.951936	6088.935076	15.451955	-0.048469	4.219854
235.941761	6080.946714	15.456960	-0.048462	4.217187
235.848631	6072.953789	15.461965	-0.048440	4.214515
235.814225	6064.926844	15.466970	-0.048428	4.211831
235.833999	6056.922032	15.471975	-0.048427	4.209153
235.716966	6048.954511	15.476979	-0.048400	4.206485
235.875312	6040.932290	15.481984	-0.048425	4.203799
235.584028	6032.988803	15.486989	-0.048365	4.201134
235.669829	6024.929735	15.491994	-0.048376	4.198432
235.935245	6016.952901	15.496999	-0.048421	4.195757
235.822376	6008.850923	15.502003	-0.048395	4.193035
235.604017	6000.813367	15.507008	-0.048349	4.190332
235.724285	5992.862052	15.512013	-0.048366	4.187660
235.606723	5984.880825	15.517018	-0.048339	4.184973
235.436584	5976.936157	15.522023	-0.048303	4.182296
235.508092	5968.873848	15.527027	-0.048311	4.179581
235.644723	5960.947911	15.532032	-0.048332	4.176910
235.572437	5952.912744	15.537037	-0.048313	4.174198
235.432441	5944.866607	15.542042	-0.048282	4.171481
235.279858	5936.928758	15.547047	-0.048249	4.168798
235.257742	5928.901190	15.552051	-0.048239	4.166084
235.250641	5920.894967	15.557056	-0.048233	4.163376
235.082024	5912.912398	15.562061	-0.048197	4.160672
235.024794	5904.932183	15.567066	-0.048181	4.157969
235.093025	5896.900356	15.572071	-0.048189	4.155248
234.969396	5888.885966	15.577075	-0.048161	4.152529
234.970375	5880.846772	15.582080	-0.048156	4.149801
234.899990	5872.882477	15.587085	-0.048138	4.147095
234.853782	5864.844486	15.592090	-0.048124	4.144364
234.977960	5856.936104	15.597095	-0.048142	4.141676
234.795389	5848.890588	15.602099	-0.048103	4.138937
234.852303	5840.940876	15.607104	-0.048109	4.136231
234.557219	5832.878070	15.612109	-0.048049	4.133480
234.659330	5824.859425	15.617114	-0.048063	4.130748
234.746664	5816.871292	15.622119	-0.048074	4.128024
234.740699	5808.862572	15.627123	-0.048068	4.125290
234.715446	5800.930235	15.632128	-0.048058	4.122580
234.554274	5792.901347	15.637133	-0.048023	4.119834
234.391413	5784.920834	15.642138	-0.047988	4.117102
234.661947	5776.896616	15.647143	-0.048033	4.114359
234.419975	5768.861421	15.652147	-0.047983	4.111604
234.403690	5760.866880	15.657152	-0.047975	4.108864
234.254444	5752.866369	15.662157	-0.047943	4.106118
234.604938	5744.871250	15.667162	-0.048003	4.103379
234.463722	5736.919329	15.672167	-0.047972	4.100646
234.184898	5728.926327	15.677171	-0.047915	4.097895
234.398413	5720.927855	15.682176	-0.047949	4.095148
234.360422	5712.877374	15.687181	-0.047937	4.092377
234.085308	5704.865238	15.692186	-0.047881	4.089614
234.264191	5696.925873	15.697191	-0.047909	4.086881
234.268540	5688.911777	15.702195	-0.047905	4.084118
234.082954	5680.979414	15.707200	-0.047866	4.081378
233.883965	5672.939107	15.712205	-0.047824	4.078599
234.028847	5664.953773	15.717210	-0.047845	4.075842
233.909228	5656.923997	15.722215	-0.047818	4.073064
233.856685	5648.899739	15.727219	-0.047803	4.070287
234.118387	5640.928565	15.732224	-0.047847	4.067531
233.876876	5632.904041	15.737229	-0.047797	4.064748
233.717167	5624.951067	15.742234	-0.047762	4.061988
233.837199	5616.947022	15.747239	-0.047780	4.059213
233.924340	5608.954269	15.752243	-0.047791	4.056439
233.872303	5600.942220	15.757248	-0.047776	4.053655
233.646948	5592.890009	15.762253	-0.047729	4.050853
233.806386	5584.937599	15.767258	-0.047754	4.048088
233.688771	5576.934157	15.772263	-0.047727	4.045300
233.510370	5568.977396	15.777267	-0.047689	4.042526
233.534044	5560.936078	15.782272	-0.047688	4.039723
233.643930	5552.971787	15.787277	-0.047704	4.036946
233.571454	5544.916199	15.792282	-0.047685	4.034133
233.377232	5536.831338	15.797287	-0.047644	4.031306
233.398961	5528.851759	15.802291	-0.047643	4.028516
233.388961	5520.888011	15.807296	-0.047636	4.025730
233.142901	5512.920533	15.812301	-0.047585	4.022937
233.175258	5504.928608	15.817306	-0.047586	4.020138
233.186529	5496.965433	15.822311	-0.047584	4.017347
233.304946	5488.883819	15.827315	-0.047601	4.014514
233.229819	5480.904522	15.832320	-0.047582	4.011711
233.197721	5472.862280	15.837325	-0.047571	4.008886
233.038874	5464.902458	15.842330	-0.047536	4.006085
233.019999	5456.929524	15.847335	-0.047527	4.003280
233.181674	5448.899028	15.852339	-0.047553	4.000455
232.895950	5440.968967	15.857344	-0.047494	3.997657
232.695378	5432.946845	15.862349	-0.047452	3.994826
233.012643	5424.902255	15.867354	-0.047506	3.991993
232.896668	5416.886800	15.872359	-0.047479	3.989161
232.809443	5408.920810	15.877363	-0.047458	3.986345
232.759496	5400.933156	15.882368	-0.047444	3.983521
232.663133	5392.965716	15.887373	-0.047421	3.980700
232.595476	5384.962954	15.892378	-0.047403	3.977866
232.584213	5376.948297	15.897383	-0.047396	3.975026
232.698093	5368.913207	15.902387	-0.047412	3.972179
232.700647	5360.918157	15.907392	-0.047408	3.969342
232.466951	5352.958566	15.912397	-0.047359	3.966512
232.397877	5344.986329	15.917402	-0.047342	3.963678
232.443995	5336.992341	15.922407	-0.047345	3.960837
232.249807	5328.987625	15.927411	-0.047304	3.957985
232.347059	5321.017570	15.932416	-0.047317	3.955149
232.311685	5312.937922	15.937421	-0.047306	3.952269
232.123465	5304.919794	15.942426	-0.047265	3.949406
231.969841	5296.972331	15.947431	-0.047232	3.946568
232.122637	5288.963992	15.952435	-0.047255	3.943710
232.368665	5280.972504	15.957440	-0.047296	3.940859
232.065206	5272.989570	15.962445	-0.047235	3.937998
232.100352	5265.001785	15.967450	-0.047236	3.935140
232.274657	5256.963162	15.972455	-0.047264	3.932264
232.054233	5248.931907	15.977459	-0.047218	3.929382
232.010910	5241.012559	15.982464	-0.047204	3.926540
231.744318	5232.998119	15.987469	-0.047150	3.923659
231.677220	5225.015164	15.992474	-0.047132	3.920790
231.742887	5217.034783	15.997479	-0.047140	3.917922
231.657509	5208.975137	16.002483	-0.047119	3.915021
231.931080	5200.988869	16.007488	-0.047165	3.912151
231.644536	5192.963634	16.012493	-0.047106	3.909255
231.546485	5184.999629	16.017498	-0.047083	3.906382
231.587809	5176.997955	16.022503	-0.047086	3.903495
231.553800	5169.000070	16.027507	-0.047074	3.900607
231.427180	5161.031983	16.032512	-0.047046	3.897725
231.419686	5152.988501	16.037517	-0.047039	3.894816
231.357696	5144.968574	16.042522	-0.047023	3.891913
231.482069	5136.981848	16.047527	-0.047041	3.889023
231.410724	5128.984723	16.052531	-0.047023	3.886123
231.305552	5121.011758	16.057536	-0.046998	3.883229
231.160546	5113.004789	16.062541	-0.046966	3.880320
231.216432	5105.034336	16.067546	-0.046971	3.877426
231.302566	5097.007230	16.072551	-0.046983	3.874510
231.143871	5088.749755	16.077555	-0.046948	3.871503
230.855556	5080.878692	16.082560	-0.046889	3.868632
230.825744	5072.894149	16.087565	-0.046879	3.865722
230.857396	5064.938807	16.092570	-0.046880	3.862822
230.761446	5056.973347	16.097575	-0.046857	3.859913
230.532065	5049.000779	16.102579	-0.046809	3.856997
230.872045	5040.985782	16.107584	-0.046867	3.854075
230.665285	5032.965250	16.112589	-0.046824	3.851138
230.630455	5024.977171	16.117594	-0.046812	3.848213
230.756552	5016.984489	16.122599	-0.046831	3.845288
230.510607	5009.036579	16.127603	-0.046780	3.842370
230.584270	5001.047063	16.132608	-0.046789	3.839440
230.618257	4993.060759	16.137613	-0.046790	3.836509
230.739508	4985.030588	16.142618	-0.046808	3.833561
230.572421	4977.029726	16.147623	-0.046771	3.830616
230.245732	4969.029782	16.152627	-0.046706	3.827666
230.520594	4961.026303	16.157632	-0.046752	3.824724
230.414987	4953.080354	16.162637	-0.046727	3.821793
230.445351	4945.088718	16.167642	-0.046728	3.818847
230.349913	4937.066551	16.172647	-0.046705	3.815883
230.242964	4929.062313	16.177651	-0.046680	3.812924
230.050907	4921.062540	16.182656	-0.046639	3.809963
229.941720	4913.091230	16.187661	-0.046614	3.807011
230.129994	4905.051416	16.192666	-0.046644	3.804039
230.071313	4897.163708	16.197671	-0.046628	3.801114
229.884945	4889.117955	16.202675	-0.046588	3.798127
229.937711	4881.118289	16.207680	-0.046593	3.795159
230.044862	4873.059460	16.212685	-0.046608	3.792168
229.765959	4865.044209	16.217690	-0.046551	3.789182
229.909304	4857.056315	16.222695	-0.046573	3.786214
229.986678	4849.076908	16.227699	-0.046582	3.783245
229.917332	4841.092456	16.232704	-0.046564	3.780269
229.783899	4833.124891	16.237709	-0.046535	3.777295
229.750710	4825.087354	16.242714	-0.046523	3.774294
229.595603	4817.092039	16.247719	-0.046490	3.771305
229.315723	4809.079011	16.252723	-0.046432	3.768303
229.417798	4801.100881	16.257728	-0.046446	3.765321
229.368520	4793.139144	16.262733	-0.046432	3.762339
229.267371	4785.094481	16.267738	-0.046408	3.759323
229.284207	4777.173053	16.272743	-0.046407	3.756353
229.218001	4769.100036	16.277747	-0.046389	3.753322
229.331398	4761.068128	16.282752	-0.046405	3.750308
229.576003	4753.094243	16.287757	-0.046446	3.747316
229.501821	4745.054448	16.292762	-0.046427	3.744290
229.399521	4737.143975	16.297767	-0.046403	3.741309
229.143653	4729.141832	16.302771	-0.046350	3.738288
229.357524	4721.139014	16.307776	-0.046385	3.735275
229.157672	4713.128203	16.312781	-0.046343	3.732247
229.254882	4705.087797	16.317786	-0.046356	3.729213
228.927322	4697.171730	16.322791	-0.046290	3.726213
228.913759	4689.140692	16.327795	-0.046283	3.723174
228.946285	4681.175089	16.332800	-0.046284	3.720159
228.803234	4673.186028	16.337805	-0.046252	3.717128
228.698814	4665.200242	16.342810	-0.046228	3.714097
228.906280	4657.126067	16.347815	-0.046261	3.711037
228.589708	4649.117053	16.352819	-0.046197	3.707987
228.863987	4641.123177	16.357824	-0.046243	3.704955
228.788268	4633.170839	16.362829	-0.046224	3.701927
228.715145	4625.195374	16.367834	-0.046206	3.698888
228.582876	4617.239384	16.372839	-0.046176	3.695852
228.407453	4609.210201	16.377843	-0.046138	3.692785
228.498827	4601.190617	16.382848	-0.046150	3.689726
228.493077	4593.217560	16.387853	-0.046144	3.686680
228.361423	4585.190899	16.392858	-0.046115	3.683607
228.502765	4577.221337	16.397863	-0.046136	3.680561
228.404383	4569.231940	16.402867	-0.046113	3.677498
228.378882	4561.250885	16.407872	-0.046103	3.674438
228.461330	4553.221265	16.412877	-0.046113	3.671359
228.232043	4545.207133	16.417882	-0.046066	3.668276
228.291528	4537.203909	16.422887	-0.046072	3.665202
228.218365	4529.239883	16.427891	-0.046053	3.662136
228.111165	4521.247584	16.432896	-0.046028	3.659057
227.872868	4513.300146	16.437901	-0.045979	3.655988
227.908400	4505.254211	16.442906	-0.045980	3.652887
227.930839	4497.258850	16.447911	-0.045979	3.649802
227.811154	4489.255764	16.452915	-0.045952	3.646707
227.839010	4481.262289	16.457920	-0.045952	3.643618
227.907615	4473.265516	16.462925	-0.045960	3.640525
227.766269	4465.313414	16.467930	-0.045929	3.637442
227.656404	4457.311188	16.472935	-0.045903	3.634337
227.544227	4449.236374	16.477939	-0.045877	3.631202
227.828783	4441.247798	16.482944	-0.045925	3.628108
227.566558	4433.250379	16.487949	-0.045872	3.624993
227.394482	4425.290540	16.492954	-0.045835	3.621893
227.535992	4417.317933	16.497959	-0.045856	3.618793
227.521237	4409.305455	16.502963	-0.045848	3.615671
227.461567	4401.333499	16.507968	-0.045832	3.612561
227.371774	4393.293016	16.512973	-0.045810	3.609421
227.347785	4385.336383	16.517978	-0.045801	3.606312
227.295017	4377.346375	16.522983	-0.045786	3.603187
227.136688	4369.350940	16.527987	-0.045752	3.600054
227.434188	4361.399169	16.532992	-0.045802	3.596948
227.300993	4353.371267	16.537997	-0.045772	3.593798
227.321887	4345.323448	16.543002	-0.045771	3.590641
227.213759	4337.393758	16.548007	-0.045746	3.587525
227.263566	4329.356336	16.553011	-0.045750	3.584367
227.228636	4321.419407	16.558016	-0.045739	3.581244
227.115178	4313.396064	16.563021	-0.045713	3.578082
226.968413	4305.405271	16.568026	-0.045680	3.574929
226.972092	4297.410574	16.573031	-0.045676	3.571777
226.880418	4289.368283	16.578035	-0.045654	3.568599
226.869694	4281.409382	16.583040	-0.045647	3.565454
226.830271	4273.446216	16.588045	-0.045634	3.562304
226.537201	4265.444247	16.593050	-0.045575	3.559129
226.651437	4257.487064	16.598055	-0.045591	3.555980
226.562786	4249.367032	16.603059	-0.045570	3.552758
226.419287	4241.348932	16.608064	-0.045538	3.549571
226.333039	4233.373098	16.613069	-0.045517	3.546401
226.438819	4225.361779	16.618074	-0.045531	3.543219
226.330197	4217.423928	16.623079	-0.045506	3.540057
226.077742	4209.442172	16.628083	-0.045454	3.536870
226.350324	4201.424124	16.633088	-0.045500	3.533682
226.140322	4193.438820	16.638093	-0.045456	3.530489
226.126621	4185.439672	16.643098	-0.045448	3.527294
226.340252	4177.430466	16.648103	-0.045483	3.524099
226.321713	4169.466441	16.653107	-0.045475	3.520912
226.170222	4161.530728	16.658112	-0.045442	3.517730
226.289551	4153.488060	16.663117	-0.045459	3.514510
226.059854	4145.478793	16.668122	-0.045411	3.511289
225.960150	4137.500370	16.673127	-0.045387	3.508082
225.855412	4129.493193	16.678131	-0.045363	3.504861
226.198101	4121.542514	16.683136	-0.045422	3.501673
225.994751	4113.542943	16.688141	-0.045379	3.498445
225.747759	4105.534896	16.693146	-0.045328	3.495210
226.061524	4097.547050	16.698151	-0.045381	3.491997
225.884142	4089.523727	16.703155	-0.045343	3.488752
225.601411	4081.606561	16.708160	-0.045286	3.485543
225.471634	4073.619988	16.713165	-0.045256	3.482308
225.763828	4065.559834	16.718170	-0.045306	3.479054
225.661308	4057.637626	16.723175	-0.045282	3.475840
225.552400	4049.594075	16.728179	-0.045256	3.472573
225.660860	4041.565466	16.733184	-0.045272	3.469317
225.423195	4033.587277	16.738189	-0.045222	3.466066
225.335839	4025.583973	16.743194	-0.045201	3.462808
225.667532	4017.616013	16.748199	-0.045258	3.459574
225.190215	4009.649829	16.753203	-0.045164	3.456311
225.086347	4001.656002	16.758208	-0.045140	3.453047
225.134426	3993.595641	16.763213	-0.045144	3.449757
225.127842	3985.629056	16.768218	-0.045137	3.446500
225.184392	3977.670994	16.773223	-0.045143	3.443246
225.108166	3969.639017	16.778227	-0.045124	3.439954
225.131517	3961.712476	16.783232	-0.045123	3.436706
225.036311	3953.698904	16.788237	-0.045100	3.433415
224.977544	3945.671089	16.793242	-0.045084	3.430116
224.968849	3937.686396	16.798247	-0.045078	3.426833
225.031077	3929.648178	16.803251	-0.045084	3.423527
224.986210	3921.706066	16.808256	-0.045071	3.420254
225.001244	3913.693220	16.813261	-0.045069	3.416951
224.991166	3905.706832	16.818266	-0.045062	3.413655
224.772518	3897.714494	16.823271	-0.045016	3.410346
224.811930	3889.734980	16.828275	-0.045019	3.407048
224.526599	3881.752541	16.833280	-0.044960	3.403734
224.678517	3873.785180	16.838285	-0.044984	3.400439
224.343463	3865.809807	16.843290	-0.044916	3.397120
224.501107	3857.770980	16.848295	-0.044941	3.393788
224.493275	3849.689309	16.853299	-0.044934	3.390430
224.268396	3841.770492	16.858304	-0.044887	3.387128
224.343723	3833.747200	16.863309	-0.044896	3.383791
224.350404	3825.770551	16.868314	-0.044893	3.380467
224.185261	3817.843261	16.873319	-0.044857	3.377154
224.005891	3809.826399	16.878323	-0.044818	3.373800
224.359307	3801.782624	16.883328	-0.044879	3.370450
224.214018	3793.834047	16.888333	-0.044847	3.367120
224.066627	3785.827278	16.893338	-0.044815	3.363761
224.113185	3777.879662	16.898343	-0.044818	3.360431
224.107095	3769.891643	16.903347	-0.044812	3.357078
223.939585	3761.884673	16.908352	-0.044776	3.353709
223.857670	3753.868790	16.913357	-0.044756	3.350335
224.050151	3745.854308	16.918362	-0.044787	3.346969
223.880942	3737.891048	16.923367	-0.044750	3.343607
223.605665	3729.910336	16.928371	-0.044694	3.340231
223.778258	3721.934252	16.933376	-0.044721	3.336870
223.771451	3713.926428	16.938381	-0.044715	3.333485
223.636538	3705.895184	16.943386	-0.044685	3.330083
223.566788	3697.936496	16.948391	-0.044667	3.326710
223.358956	3689.975244	16.953395	-0.044623	3.323327
223.518782	3681.964053	16.958400	-0.044648	3.319933
223.383425	3674.022319	16.963405	-0.044618	3.316555
223.498146	3665.963869	16.968410	-0.044634	3.313132
223.262773	3657.989478	16.973415	-0.044585	3.309729
223.106033	3649.996639	16.978419	-0.044551	3.306317
223.371087	3641.981121	16.983424	-0.044595	3.302908
223.144388	3634.035947	16.988429	-0.044548	3.299507
222.994553	3626.068835	16.993434	-0.044515	3.296096
222.947601	3618.056332	16.998439	-0.044501	3.292666
223.129561	3610.016328	17.003443	-0.044530	3.289229
222.909892	3602.076134	17.008448	-0.044484	3.285816
222.838292	3594.099670	17.013453	-0.044466	3.282390
222.871123	3586.106873	17.018458	-0.044467	3.278957
222.852498	3578.137257	17.023463	-0.044459	3.275528
222.669252	3570.112688	17.028467	-0.044420	3.272066
222.816183	3562.095597	17.033472	-0.044442	3.268616
222.854916	3554.085928	17.038477	-0.044444	3.265162
222.672841	3546.130917	17.043482	-0.044405	3.261719
222.577429	3538.183673	17.048487	-0.044383	3.258278
222.483099	3530.151781	17.053491	-0.044360	3.254798
222.764276	3522.125657	17.058496	-0.044407	3.251331
222.644193	3514.168701	17.063501	-0.044380	3.247875
222.625830	3506.146925	17.068506	-0.044372	3.244391
222.554368	3498.235596	17.073511	-0.044353	3.240949
222.290273	3490.263825	17.078515	-0.044299	3.237469
222.225341	3482.260750	17.083520	-0.044282	3.233980
222.327815	3474.153445	17.088525	-0.044296	3.230448
222.120537	3466.176075	17.093530	-0.044252	3.226957
222.139321	3458.214846	17.098535	-0.044251	3.223478
222.035736	3450.237309	17.103539	-0.044227	3.219983
222.106095	3442.293461	17.108544	-0.044235	3.216507
221.869728	3434.288849	17.113549	-0.044186	3.212987
221.956408	3426.247724	17.118554	-0.044197	3.209461
222.130857	3418.302953	17.123559	-0.044224	3.205976
221.932739	3410.343159	17.128563	-0.044183	3.202466
221.840276	3402.346741	17.133568	-0.044160	3.198941
221.968761	3394.353033	17.138573	-0.044179	3.195422
221.804077	3386.339460	17.143578	-0.044144	3.191877
221.900276	3378.370682	17.148583	-0.044156	3.188360
221.743164	3370.349548	17.153587	-0.044122	3.184805
221.825231	3362.399062	17.158592	-0.044133	3.181288
221.494327	3354.450560	17.163597	-0.044066	3.177749
221.692379	3346.386342	17.168602	-0.044098	3.174179
221.756629	3338.406505	17.173607	-0.044105	3.170635
221.748505	3330.408185	17.178611	-0.044098	3.167077
221.230542	3322.475245	17.183616	-0.043997	3.163522
221.181714	3314.482162	17.188621	-0.043983	3.159956
221.323807	3306.485157	17.193626	-0.044004	3.156392
221.296414	3298.498266	17.198631	-0.043994	3.152822
221.090252	3290.471634	17.203635	-0.043951	3.149222
221.066787	3282.485180	17.208640	-0.043941	3.145644
221.096716	3274.542952	17.213645	-0.043942	3.142084
221.093979	3266.517699	17.218650	-0.043936	3.138481
221.261156	3258.569645	17.223655	-0.043963	3.134916
220.910715	3250.566467	17.228659	-0.043892	3.131300
220.696914	3242.588999	17.233664	-0.043847	3.127697
221.145284	3234.556679	17.238669	-0.043926	3.124094
220.969496	3226.624322	17.243674	-0.043888	3.120505
220.844662	3218.677482	17.248679	-0.043860	3.116907
220.626483	3210.648515	17.253683	-0.043814	3.113264
220.738602	3202.637431	17.258688	-0.043830	3.109639
220.719717	3194.652166	17.263693	-0.043822	3.106016
220.386401	3186.704278	17.268698	-0.043755	3.102391
220.573871	3178.714287	17.273703	-0.043785	3.098767
220.272746	3170.738112	17.278707	-0.043724	3.095122
220.388932	3162.725350	17.283712	-0.043740	3.091476
220.417744	3154.735588	17.288717	-0.043741	3.087831
220.367000	3146.720944	17.293722	-0.043726	3.084168
220.293393	3138.786384	17.298727	-0.043707	3.080535
220.301729	3130.786131	17.303731	-0.043704	3.076872
220.378505	3122.753056	17.308736	-0.043713	3.073193
220.287799	3114.703801	17.313741	-0.043691	3.069494
220.264082	3106.751830	17.318746	-0.043682	3.065838
220.370191	3098.803541	17.323751	-0.043697	3.062186
220.280507	3090.829201	17.328755	-0.043675	3.058509
220.053446	3082.875218	17.333760	-0.043628	3.054829
219.877267	3074.889893	17.338765	-0.043590	3.051134
219.867548	3066.868166	17.343770	-0.043583	3.047424
219.817076	3058.918385	17.348775	-0.043569	3.043742
219.759799	3050.943949	17.353779	-0.043553	3.040043
219.912139	3042.975685	17.358784	-0.043576	3.036353
219.820443	3034.962447	17.363789	-0.043554	3.032626
219.685440	3026.956906	17.368794	-0.043524	3.028895
219.806768	3018.986844	17.373799	-0.043542	3.025189
219.872277	3010.991501	17.378803	-0.043549	3.021464
219.579039	3003.030135	17.383808	-0.043489	3.017732
219.544455	2995.061682	17.388813	-0.043478	3.014006
219.610532	2987.016547	17.393818	-0.043485	3.010243
219.733944	2979.057297	17.398823	-0.043503	3.006519
219.311410	2971.105512	17.403827	-0.043420	3.002767
219.305202	2963.121277	17.408832	-0.043413	2.999016
219.354676	2955.163701	17.413837	-0.043418	2.995275
219.100349	2947.125670	17.418842	-0.043365	2.991477
219.200691	2939.148338	17.423847	-0.043379	2.987720
219.008168	2931.154637	17.428851	-0.043338	2.983936
218.939982	2923.198190	17.433856	-0.043320	2.980170
218.944123	2915.236208	17.438861	-0.043316	2.976401
218.864708	2907.216886	17.443866	-0.043296	2.972596
218.998897	2899.217871	17.448871	-0.043316	2.968807
218.768679	2891.245112	17.453875	-0.043269	2.965007
218.978668	2883.273419	17.458880	-0.043303	2.961224
218.890093	2875.303999	17.463885	-0.043281	2.957423
218.778671	2867.312672	17.468890	-0.043255	2.953605
218.814364	2859.310617	17.473895	-0.043257	2.949785
218.923100	2851.322747	17.478899	-0.043272	2.945970
218.551447	2843.384876	17.483904	-0.043198	2.942149
218.733728	2835.380427	17.488909	-0.043227	2.938320
218.807282	2827.384502	17.493914	-0.043236	2.934485
218.790701	2819.399731	17.498919	-0.043228	2.930645
218.574604	2811.427132	17.503923	-0.043183	2.926796
218.523272	2803.460703	17.508928	-0.043168	2.922953
218.518367	2795.500984	17.513933	-0.043162	2.919111
218.198588	2787.547582	17.518938	-0.043098	2.915250
218.191966	2779.479553	17.523943	-0.043091	2.911345
218.230369	2771.459238	17.528947	-0.043093	2.907460
218.174291	2763.486408	17.533952	-0.043078	2.903588
217.978399	2755.571803	17.538957	-0.043037	2.899732
218.039477	2747.570122	17.543962	-0.043043	2.895842
218.059108	2739.591443	17.548967	-0.043042	2.891955
218.100374	2731.583983	17.553971	-0.043044	2.888051
218.113147	2723.603274	17.558976	-0.043042	2.884153
217.882145	2715.689868	17.563981	-0.042994	2.880269
217.569580	2707.718670	17.568986	-0.042930	2.876347
217.799329	2699.700371	17.573991	-0.042968	2.872427
217.765532	2691.686869	17.578995	-0.042957	2.868489
217.748278	2683.699657	17.584000	-0.042949	2.864559
217.621192	2675.775038	17.589005	-0.042920	2.860649
217.473724	2667.790246	17.594010	-0.042888	2.856702
217.604302	2659.804767	17.599015	-0.042907	2.852765
217.548142	2651.795844	17.604019	-0.042892	2.848801
217.395148	2643.848119	17.609024	-0.042858	2.844856
217.679932	2635.854289	17.614029	-0.042906	2.840907
217.365197	2627.911906	17.619034	-0.042843	2.836945
217.313025	2619.938357	17.624039	-0.042828	2.832976
217.199682	2611.919721	17.629043	-0.042802	2.828976
217.233877	2603.926284	17.634048	-0.042803	2.824991
217.225569	2595.973330	17.639053	-0.042797	2.821018
217.056812	2588.000695	17.644058	-0.042760	2.817021
216.850925	2580.044976	17.649063	-0.042717	2.813024
216.959140	2572.011692	17.654067	-0.042732	2.809001
217.046649	2564.018326	17.659072	-0.042743	2.804990
217.131747	2556.077551	17.664077	-0.042754	2.801001
216.793722	2548.120149	17.669082	-0.042686	2.796973
216.896726	2540.138185	17.674087	-0.042700	2.792952
216.697736	2532.150804	17.679091	-0.042658	2.788905
216.930305	2524.134868	17.684096	-0.042697	2.784863
217.009953	2516.187019	17.689101	-0.042706	2.780840
216.825104	2508.231031	17.694106	-0.042667	2.776792
216.726285	2500.269338	17.699111	-0.042644	2.772740
216.543155	2492.278926	17.704115	-0.042605	2.768663
216.398447	2484.298945	17.709120	-0.042573	2.764587
216.592441	2476.338756	17.714125	-0.042604	2.760536
216.330017	2468.383348	17.719130	-0.042550	2.756454
216.422712	2460.345672	17.724135	-0.042562	2.752344
216.291562	2452.317125	17.729139	-0.042533	2.748220
216.330235	2444.346873	17.734144	-0.042535	2.744130
216.194927	2436.413303	17.739149	-0.042505	2.740042
216.101149	2428.433422	17.744154	-0.042482	2.735927
216.006193	2420.460899	17.749159	-0.042460	2.731809
216.022498	2412.466693	17.754163	-0.042458	2.727680
216.002311	2404.516660	17.759168	-0.042449	2.723566
215.983484	2396.559822	17.764173	-0.042440	2.719442
215.793901	2388.624031	17.769178	-0.042400	2.715312
215.878853	2380.612958	17.774183	-0.042411	2.711154
215.642877	2372.630997	17.779187	-0.042362	2.706985
215.934598	2364.623874	17.784192	-0.042411	2.702829
216.006086	2356.664330	17.789197	-0.042420	2.698677
215.784172	2348.721886	17.794202	-0.042373	2.694510
215.663475	2340.753441	17.799207	-0.042346	2.690329
215.541539	2332.772027	17.804211	-0.042318	2.686135
215.376880	2324.826127	17.809216	-0.042283	2.681950
215.361224	2316.861626	17.814221	-0.042275	2.677758
215.522177	2308.850289	17.819226	-0.042300	2.673546
215.507515	2300.833821	17.824231	-0.042292	2.669313
215.094542	2292.912193	17.829235	-0.042210	2.665099
215.337954	2284.897379	17.834240	-0.042250	2.660870
215.287120	2276.975795	17.839245	-0.042236	2.656666
214.867809	2269.001448	17.844250	-0.042153	2.652402
214.959546	2261.027684	17.849255	-0.042165	2.648166
214.944578	2253.023524	17.854259	-0.042157	2.643899
214.935841	2245.065710	17.859264	-0.042151	2.639650
215.036364	2237.111637	17.864269	-0.042164	2.635404
214.998396	2229.092153	17.869274	-0.042152	2.631107
214.985849	2221.145167	17.874279	-0.042145	2.626844
214.508681	2213.226157	17.879283	-0.042051	2.622557
214.716978	2205.228806	17.884288	-0.042085	2.618267
214.592526	2197.270088	17.889293	-0.042057	2.613969
214.379977	2189.279145	17.894298	-0.042012	2.609640
214.409360	2181.313582	17.899303	-0.042013	2.605334
214.575941	2173.333704	17.904307	-0.042039	2.601022
214.468063	2165.400062	17.909312	-0.042014	2.596710
214.475843	2157.304220	17.914317	-0.042010	2.592310
214.389576	2149.236752	17.919322	-0.041989	2.587912
214.289612	2141.340048	17.924327	-0.041965	2.583599
214.217851	2133.409363	17.929331	-0.041947	2.579261
214.043246	2125.475920	17.934336	-0.041910	2.574908
214.054362	2117.489632	17.939341	-0.041907	2.570531
214.010873	2109.513031	17.944346	-0.041894	2.566148
213.962519	2101.594360	17.949351	-0.041880	2.561789
214.045233	2093.623631	17.954355	-0.041890	2.557404
214.165088	2085.632706	17.959360	-0.041907	2.553002
214.166450	2077.663755	17.964365	-0.041903	2.548596
213.980048	2069.694993	17.969370	-0.041863	2.544170
213.798896	2061.790700	17.974375	-0.041824	2.539772
213.640724	2053.825431	17.979379	-0.041790	2.535334
213.783472	2045.813359	17.984384	-0.041811	2.530883
213.820795	2037.854497	17.989389	-0.041813	2.526447
213.757183	2029.886224	17.994394	-0.041797	2.521991
213.669438	2021.964143	17.999399	-0.041775	2.517551
213.652571	2013.956297	18.004403	-0.041767	2.513060
213.477380	2005.980642	18.009408	-0.041730	2.508567
213.400674	1998.025809	18.014413	-0.041710	2.504086
213.378189	1990.051423	18.019418	-0.041701	2.499589
213.355272	1982.125419	18.024423	-0.041692	2.495112
213.266386	1974.132595	18.029427	-0.041670	2.490583
213.249361	1966.162375	18.034432	-0.041662	2.486065
213.260851	1958.218878	18.039437	-0.041659	2.481555
213.306037	1950.251702	18.044442	-0.041663	2.477027
213.213764	1942.313400	18.049447	-0.041641	2.472496
213.135099	1934.311986	18.054451	-0.041621	2.467922
212.856408	1926.370926	18.059456	-0.041564	2.463359
212.665065	1918.436590	18.064461	-0.041523	2.458798
212.838410	1910.440257	18.069466	-0.041551	2.454220
212.715189	1902.489222	18.074471	-0.041523	2.449638
212.877637	1894.507491	18.079475	-0.041548	2.445050
212.686519	1886.568772	18.084480	-0.041508	2.440452
212.545807	1878.637409	18.089485	-0.041476	2.435854
212.532649	1870.587758	18.094490	-0.041469	2.431188
212.506542	1862.622683	18.099495	-0.041459	2.426561
212.492482	1854.658883	18.104499	-0.041451	2.421926
212.453372	1846.710970	18.109504	-0.041439	2.417291
212.334890	1838.775767	18.114509	-0.041412	2.412647
212.440307	1830.778179	18.119514	-0.041427	2.407976
212.431961	1822.835912	18.124519	-0.041420	2.403319
212.307790	1814.894208	18.129523	-0.041392	2.398644
212.078699	1806.981265	18.134528	-0.041345	2.393969
212.229110	1798.973163	18.139533	-0.041368	2.389258
211.894106	1791.035696	18.144538	-0.041300	2.384542
211.927216	1783.090606	18.149543	-0.041301	2.379841
211.957308	1775.131885	18.154547	-0.041302	2.375122
211.787288	1767.168369	18.159552	-0.041265	2.370375
211.758792	1759.219395	18.164557	-0.041255	2.365638
211.518456	1751.278329	18.169562	-0.041205	2.360879
211.720926	1743.321537	18.174567	-0.041238	2.356137
211.544145	1735.350963	18.179571	-0.041200	2.351347
211.459446	1727.374400	18.184576	-0.041179	2.346551
211.683595	1719.399268	18.189581	-0.041216	2.341771
211.519413	1711.451606	18.194586	-0.041181	2.336966
211.412854	1703.523135	18.199591	-0.041156	2.332167
211.414291	1695.540183	18.204595	-0.041151	2.327334
211.598965	1687.578116	18.209600	-0.041181	2.322519
211.485861	1679.663341	18.214605	-0.041155	2.317698
211.268059	1671.721051	18.219610	-0.041109	2.312842
211.271868	1663.756545	18.224615	-0.041105	2.307980
210.928601	1655.818421	18.229619	-0.041036	2.303095
210.767222	1647.897308	18.234624	-0.041001	2.298226
211.031648	1639.900261	18.239629	-0.041045	2.293335
211.037176	1631.920023	18.244634	-0.041041	2.288422
210.742663	1624.030881	18.249639	-0.040981	2.283529
210.946173	1616.054000	18.254643	-0.041014	2.278614
210.974852	1608.076332	18.259648	-0.041015	2.273673
210.822710	1600.083261	18.264653	-0.040981	2.268696
210.472137	1592.163146	18.269658	-0.040911	2.263737
210.535827	1584.223338	18.274663	-0.040918	2.258790
210.476646	1576.265322	18.279667	-0.040902	2.253810
210.649993	1568.275869	18.284672	-0.040929	2.248820
210.669751	1560.354236	18.289677	-0.040928	2.243847
210.595087	1552.411286	18.294682	-0.040909	2.238842
210.405709	1544.514287	18.299687	-0.040869	2.233845
210.500813	1536.518041	18.304691	-0.040882	2.228799
210.413662	1528.583340	18.309696	-0.040860	2.223764
210.454771	1520.661907	18.314701	-0.040863	2.218737
210.112270	1512.744449	18.319706	-0.040794	2.213668
210.131276	1504.783219	18.324711	-0.040793	2.208591
210.183752	1496.810185	18.329715	-0.040798	2.203498
209.869238	1488.920474	18.334720	-0.040734	2.198413
210.070484	1480.950590	18.339725	-0.040767	2.193312
210.043844	1472.946829	18.344730	-0.040757	2.188156
209.977144	1465.026317	18.349735	-0.040739	2.183038
209.960418	1457.090321	18.354739	-0.040731	2.177903
209.906773	1449.145103	18.359744	-0.040716	2.172746
209.687233	1441.224146	18.364749	-0.040670	2.167578
209.790511	1433.253724	18.369754	-0.040685	2.162395
209.942483	1425.316142	18.374759	-0.040708	2.157225
209.635754	1417.417751	18.379763	-0.040646	2.152025
209.563527	1409.459487	18.384768	-0.040628	2.146796
209.526505	1401.536695	18.389773	-0.040616	2.141581
209.431026	1393.597152	18.394778	-0.040593	2.136336
209.200528	1385.678394	18.399783	-0.040545	2.131079
209.272832	1377.714125	18.404787	-0.040554	2.125808
209.086758	1369.801355	18.409792	-0.040514	2.120533
209.187129	1361.864503	18.414797	-0.040528	2.115256
209.180225	1353.847040	18.419802	-0.040521	2.109903
209.132144	1345.913858	18.424807	-0.040508	2.104588
209.102571	1337.984577	18.429811	-0.040497	2.099263
208.996528	1330.069353	18.434816	-0.040472	2.093928
208.897527	1322.125960	18.439821	-0.040449	2.088560
208.903761	1314.175983	18.444826	-0.040445	2.083184
208.853139	1306.287427	18.449831	-0.040431	2.077831
208.897377	1298.343927	18.454835	-0.040434	2.072436
208.750770	1290.409111	18.459840	-0.040402	2.067013
208.659165	1282.500627	18.464845	-0.040380	2.061600
208.571631	1274.570726	18.469850	-0.040359	2.056158
208.594809	1266.618862	18.474855	-0.040358	2.050698
208.453774	1258.712228	18.479859	-0.040327	2.045238
208.293308	1250.792404	18.484864	-0.040292	2.039752
208.257786	1242.886187	18.489869	-0.040280	2.034273
208.145104	1234.906674	18.494874	-0.040254	2.028721
208.308084	1226.963710	18.499879	-0.040280	2.023207
208.089044	1219.075888	18.504883	-0.040234	2.017677
208.057708	1211.141557	18.509888	-0.040223	2.012119
207.784089	1203.240817	18.514893	-0.040167	2.006544
207.956660	1195.271056	18.519898	-0.040194	2.000951
207.948511	1187.377398	18.524903	-0.040188	1.995378
207.870374	1179.434710	18.529907	-0.040168	1.989747
207.726349	1171.532911	18.534912	-0.040137	1.984121
207.841169	1163.607153	18.539917	-0.040153	1.978490
207.795673	1155.683660	18.544922	-0.040140	1.972828
207.666612	1147.765804	18.549927	-0.040111	1.967144
207.380228	1139.893139	18.554931	-0.040052	1.961460
207.381239	1131.964745	18.559936	-0.040048	1.955750
207.337444	1124.012034	18.564941	-0.040035	1.950000
207.040557	1116.097340	18.569946	-0.039974	1.944234
207.180361	1108.166848	18.574951	-0.039995	1.938486
207.210829	1100.224221	18.579955	-0.039996	1.932701
207.027603	1092.324739	18.584960	-0.039957	1.926906
206.994003	1084.419541	18.589965	-0.039946	1.921106
206.863339	1076.525329	18.594970	-0.039917	1.915286
206.942197	1068.589891	18.599975	-0.039926	1.909441
206.664599	1060.707169	18.604979	-0.039870	1.903577
206.777086	1052.774223	18.609984	-0.039886	1.897702
206.783165	1044.864920	18.614989	-0.039882	1.891813
206.445582	1036.975497	18.619994	-0.039814	1.885883
206.550142	1029.065869	18.624999	-0.039829	1.879969
206.501889	1021.166770	18.630003	-0.039815	1.874026
206.250810	1013.244527	18.635008	-0.039763	1.868024
206.382937	1005.321703	18.640013	-0.039783	1.862046
206.281928	997.420620	18.645018	-0.039759	1.856039
206.376007	989.492552	18.650023	-0.039771	1.850014
206.212857	981.620879	18.655027	-0.039736	1.843982
206.088645	973.743052	18.660032	-0.039708	1.837931
206.095237	965.844369	18.665037	-0.039704	1.831859
205.744674	957.958545	18.670042	-0.039634	1.825734
205.682979	950.071226	18.675047	-0.039618	1.819622
205.903060	942.131808	18.680051	-0.039654	1.813482
205.808203	934.231718	18.685056	-0.039631	1.807314
205.697651	926.370034	18.690061	-0.039606	1.801154
205.571850	918.489803	18.695066	-0.039577	1.794955
205.473361	910.538418	18.700071	-0.039554	1.788683
205.558362	902.618023	18.705075	-0.039565	1.782435
205.489594	894.749185	18.710080	-0.039547	1.776188
205.579848	886.836290	18.715085	-0.039559	1.769903
205.519245	878.958691	18.720090	-0.039543	1.763605
205.300339	871.118589	18.725095	-0.039497	1.757294
205.155441	863.241963	18.730099	-0.039465	1.750941
205.240790	855.326715	18.735104	-0.039476	1.744562
205.149266	847.469916	18.740109	-0.039454	1.738185
205.121581	839.577746	18.745114	-0.039444	1.731764
204.981570	831.704209	18.750119	-0.039413	1.725320
204.847903	823.855939	18.755123	-0.039383	1.718873
204.748936	815.973942	18.760128	-0.039360	1.712378
204.929160	808.044477	18.765133	-0.039389	1.705856
204.778239	800.185327	18.770138	-0.039356	1.699324
204.651204	792.336045	18.775143	-0.039327	1.692778
204.569913	784.452495	18.780147	-0.039307	1.686184
204.591872	776.575650	18.785152	-0.039306	1.679583
204.497799	768.739755	18.790157	-0.039284	1.672975
204.302429	760.867050	18.795162	-0.039242	1.666297
204.475668	752.983247	18.800167	-0.039270	1.659631
204.484116	745.115769	18.805171	-0.039266	1.652931
204.279017	737.264056	18.810176	-0.039223	1.646187
204.233769	729.427145	18.815181	-0.039210	1.639451
204.121827	721.547095	18.820186	-0.039184	1.632640
203.854069	713.678483	18.825191	-0.039129	1.625788
203.672087	705.846715	18.830195	-0.039091	1.618952
203.881266	697.945505	18.835200	-0.039125	1.612081
203.664697	690.122385	18.840205	-0.039079	1.605189
203.442987	682.308738	18.845210	-0.039033	1.598275
203.780974	674.395207	18.850215	-0.039091	1.591322
203.499737	666.579251	18.855219	-0.039034	1.584336
203.445199	658.742948	18.860224	-0.039019	1.577335
203.570035	650.870949	18.865229	-0.039037	1.570295
203.589906	643.025569	18.870234	-0.039036	1.563233
203.334461	635.246824	18.875239	-0.038984	1.556159
203.243147	627.390181	18.880243	-0.038962	1.549006
203.401864	619.512585	18.885248	-0.038986	1.541837
203.117595	611.735640	18.890253	-0.038928	1.534662
203.075734	603.885097	18.895258	-0.038916	1.527421
203.110609	596.060598	18.900263	-0.038917	1.520181
202.907593	588.276516	18.905267	-0.038875	1.512908
202.573669	580.479738	18.910272	-0.038808	1.505568
202.557822	572.659557	18.915277	-0.038800	1.498219
202.619802	564.796829	18.920282	-0.038806	1.490805
202.525430	557.001586	18.925287	-0.038784	1.483394
202.426420	549.206719	18.930291	-0.038761	1.475946
202.473201	541.330153	18.935296	-0.038764	1.468404
202.477807	533.526999	18.940301	-0.038760	1.460887
202.112098	525.769477	18.945306	-0.038688	1.453317
202.215216	517.931075	18.950311	-0.038702	1.445704
202.041869	510.173403	18.955315	-0.038665	1.438084
201.843481	502.395568	18.960320	-0.038623	1.430400
202.074977	494.562997	18.965325	-0.038661	1.422691
201.840986	486.803586	18.970330	-0.038613	1.414936
201.674145	479.035926	18.975335	-0.038577	1.407140
201.538246	471.271289	18.980339	-0.038547	1.399310
201.597927	463.466761	18.985344	-0.038553	1.391428
201.572793	455.676259	18.990349	-0.038543	1.383501
201.179195	447.960092	18.995354	-0.038465	1.375541
201.221710	440.164775	19.000359	-0.038468	1.367529
201.261044	432.391118	19.005363	-0.038471	1.359491
200.898847	424.685547	19.010368	-0.038398	1.351406
201.030487	416.894305	19.015373	-0.038418	1.343269
201.090555	409.121371	19.020378	-0.038424	1.335090
200.867453	401.402152	19.025383	-0.038378	1.326867
200.549818	393.715650	19.030387	-0.038314	1.318610
200.665131	385.847523	19.035392	-0.038331	1.310184
200.656352	378.070110	19.040397	-0.038324	1.301779
200.571145	370.354838	19.045402	-0.038303	1.293373
200.483648	362.638538	19.050407	-0.038282	1.284911
200.601894	354.912932	19.055411	-0.038300	1.276420
200.354455	347.230940	19.060416	-0.038249	1.267853
200.333007	339.525136	19.065421	-0.038240	1.259243
200.296915	331.815423	19.070426	-0.038228	1.250567
200.195334	324.141247	19.075431	-0.038205	1.241858
200.093388	316.466572	19.080435	-0.038181	1.233087
200.146687	308.741438	19.085440	-0.038186	1.224225
200.090012	301.070193	19.090445	-0.038171	1.215339
199.780058	293.427469	19.095450	-0.038108	1.206371
199.755414	285.774023	19.100455	-0.038099	1.197380
199.624067	278.119821	19.105459	-0.038070	1.188299
199.428955	270.483800	19.110464	-0.038028	1.179156
199.315281	262.847955	19.115469	-0.038002	1.169959
199.239660	255.200436	19.120474	-0.037984	1.160682
199.258576	247.538340	19.125479	-0.037982	1.151333
199.204858	239.890505	19.130483	-0.037968	1.141909
199.248981	232.253144	19.135488	-0.037971	1.132441
199.296433	224.634011	19.140493	-0.037975	1.122917
198.751999	217.116112	19.145498	-0.037869	1.113310
198.863918	209.487635	19.150503	-0.037885	1.103623
198.873431	201.895892	19.155507	-0.037882	1.093875
198.628422	194.350512	19.160512	-0.037832	1.084042
198.623394	186.788708	19.165517	-0.037826	1.074152
198.326956	179.247528	19.170522	-0.037766	1.064130
198.357292	171.690554	19.175527	-0.037767	1.054068
198.085105	164.185657	19.180531	-0.037712	1.043908
197.917430	156.678608	19.185536	-0.037676	1.033670
197.789244	149.172940	19.190541	-0.037647	1.023341
197.807335	141.649002	19.195546	-0.037646	1.012917
197.751086	134.159447	19.200551	-0.037631	1.002414
197.709123	126.674998	19.205555	-0.037618	0.991810
197.553904	119.194529	19.210560	-0.037585	0.981070
197.636687	111.728054	19.215565	-0.037596	0.970291
197.480296	104.305523	19.220570	-0.037562	0.959394
197.552156	96.868440	19.225575	-0.037571	0.948410
197.160389	89.527504	19.230579	-0.037493	0.937320
196.827119	82.172450	19.235584	-0.037426	0.926091
197.026295	74.767676	19.240589	-0.037459	0.914791
196.668893	67.443635	19.245594	-0.037388	0.903323
196.388802	60.374396	19.250599	-0.037331	0.892132