Thu Mar 11 19:29:03 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.372291	0.024850	0.000000	0.000030	0.724273

0.393920	0.019595	0.005005	0.000026	0.724270
0.374240	0.021016	0.010010	0.000029	0.724267
0.342655	0.029261	0.015014	0.000035	0.724272
0.134812	0.062548	0.020019	0.000073	0.724265
0.301710	0.036013	0.025024	0.000042	0.724272
0.399269	0.016283	0.030029	0.000024	0.724268
0.408858	0.014447	0.035034	0.000022	0.724268
0.464751	0.007158	0.040038	0.000011	0.724273
0.618878	-0.024118	0.045043	-0.000018	0.724266
0.692411	-0.032994	0.050048	-0.000032	0.724275
0.519241	-0.005163	0.055053	0.000000	0.724270
0.774443	-0.053915	0.060058	-0.000048	0.724263
0.671988	-0.169110	0.065062	-0.000029	0.724003
0.423110	-0.151147	0.070067	0.000017	0.723951
0.515062	-0.161312	0.075072	0.000000	0.723964
0.615652	-0.181222	0.080077	-0.000019	0.723960
0.258610	-0.118183	0.085082	0.000047	0.723960
0.367953	-0.135348	0.090086	0.000027	0.723965
0.384170	-0.144580	0.095091	0.000024	0.723953
0.307284	-0.171777	0.100096	0.000038	0.723873
0.356343	-0.299617	0.105101	0.000028	0.723640
0.445499	-0.316535	0.110106	0.000012	0.723638
0.560191	-0.335014	0.115110	-0.000010	0.723643
0.365532	-0.304189	0.120115	0.000026	0.723635
0.476008	-0.320562	0.125120	0.000005	0.723642
0.405396	-0.432473	0.130125	0.000018	0.723399
0.430637	-0.464048	0.135130	0.000013	0.723346
0.441220	-0.462797	0.140134	0.000011	0.723353
0.416573	-0.463354	0.145139	0.000016	0.723343
0.408626	-0.521538	0.150144	0.000017	0.723227
0.240121	-0.600946	0.155149	0.000048	0.723013
0.250144	-0.604412	0.160154	0.000046	0.723010
0.343271	-0.617063	0.165158	0.000028	0.723018
0.367011	-0.687466	0.170163	0.000024	0.722889
0.259207	-0.762954	0.175168	0.000044	0.722703
0.351049	-0.780828	0.180173	0.000026	0.722701
0.236514	-0.762434	0.185178	0.000048	0.722697
0.176676	-0.883613	0.190182	0.000059	0.722439
0.262376	-0.934703	0.195187	0.000042	0.722369
0.285799	-0.933278	0.200192	0.000038	0.722380
-0.079903	-0.946641	0.205197	0.000106	0.722227
0.147501	-1.060667	0.210202	0.000063	0.722083
0.331594	-1.090715	0.215206	0.000029	0.722088
0.135367	-1.134143	0.220211	0.000065	0.721935
0.244176	-1.242912	0.225216	0.000045	0.721760
0.235589	-1.244730	0.230221	0.000046	0.721753
0.067704	-1.312109	0.235226	0.000077	0.721563
-0.055737	-1.348270	0.240230	0.000100	0.721449
0.101288	-1.379656	0.245235	0.000071	0.721442
0.264864	-1.542691	0.250240	0.000040	0.721180
0.276404	-1.570633	0.255245	0.000038	0.721129
0.003427	-1.568583	0.260250	0.000088	0.721038
-0.186758	-1.608487	0.265254	0.000123	0.720893
-0.662230	-1.530214	0.270259	0.000212	0.720881
-0.618146	-1.659809	0.275264	0.000203	0.720642
-0.301161	-1.763341	0.280269	0.000144	0.720550
-0.412355	-1.779713	0.285274	0.000165	0.720479
-0.395353	-1.903982	0.290278	0.000161	0.720241
-0.702824	-1.853082	0.295283	0.000218	0.720233
-0.572123	-2.004055	0.300288	0.000194	0.719982
-1.233522	-1.923720	0.305293	0.000317	0.719909
-1.226046	-1.970264	0.310298	0.000315	0.719820
-2.065565	-1.924615	0.315302	0.000471	0.719616
-1.927364	-1.953080	0.320307	0.000445	0.719609
-1.857639	-2.057133	0.325312	0.000432	0.719429
-3.203133	-1.893643	0.330317	0.000682	0.719279
-3.072509	-1.917511	0.335322	0.000658	0.719278
-2.763596	-2.046352	0.340326	0.000600	0.719133
-4.270739	-1.863134	0.345331	0.000881	0.718965
-3.809355	-1.941519	0.350336	0.000794	0.718973
-3.745054	-1.964020	0.355341	0.000782	0.718952
-4.627963	-1.960611	0.360346	0.000946	0.718649
-4.493675	-1.980663	0.365350	0.000921	0.718657
-5.031906	-1.888373	0.370355	0.001021	0.718650
-4.800590	-1.971972	0.375360	0.000978	0.718567
-5.591009	-1.931782	0.380365	0.001125	0.718369
-5.796362	-1.897946	0.385370	0.001163	0.718364
-5.700610	-1.913114	0.390374	0.001145	0.718368
-5.891009	-1.883246	0.395379	0.001180	0.718360
-6.470025	-1.937575	0.400384	0.001288	0.718050
-6.604264	-1.924819	0.405389	0.001312	0.718028
-6.715705	-1.908103	0.410394	0.001333	0.718022
-6.523827	-1.938180	0.415398	0.001297	0.718031
-7.196296	-1.823988	0.420403	0.001422	0.718020
-7.234730	-1.967729	0.425408	0.001429	0.717723
-7.535125	-1.919607	0.430413	0.001485	0.717713
-8.075132	-1.825922	0.435418	0.001585	0.717708
-7.376148	-1.947393	0.440422	0.001455	0.717715
-7.646557	-1.904532	0.445427	0.001505	0.717705
-7.938242	-1.956198	0.450432	0.001559	0.717500
-8.800487	-1.859196	0.455437	0.001719	0.717389
-8.673489	-1.884789	0.460442	0.001695	0.717383
-8.598625	-1.894740	0.465446	0.001681	0.717390
-9.105666	-1.808109	0.470451	0.001775	0.717383
-8.526301	-1.907961	0.475456	0.001667	0.717390
-8.560679	-1.976327	0.480461	0.001674	0.717244
-10.128865	-1.776244	0.485466	0.001965	0.717087
-9.088947	-1.957386	0.490470	0.001771	0.717096
-9.239101	-1.934321	0.495475	0.001799	0.717089
-9.540374	-1.879406	0.500480	0.001855	0.717092
-9.292955	-1.922936	0.505485	0.001809	0.717093
-9.619728	-1.941553	0.510490	0.001869	0.716942
-10.654097	-1.845153	0.515494	0.002062	0.716768
-10.458790	-1.884923	0.520499	0.002025	0.716759
-10.389227	-1.896143	0.525504	0.002012	0.716762
-10.702062	-1.838734	0.530509	0.002070	0.716765
-10.731596	-1.837350	0.535514	0.002075	0.716758
-10.158836	-1.935206	0.540518	0.001968	0.716767
-10.483664	-1.998288	0.545523	0.002029	0.716528
-11.379017	-1.872476	0.550528	0.002195	0.716461
-11.556497	-1.842567	0.555533	0.002228	0.716458
-11.495592	-1.856858	0.560538	0.002216	0.716452
-11.227017	-1.899665	0.565542	0.002166	0.716462
-11.475839	-1.859493	0.570547	0.002212	0.716455
-11.467130	-1.858021	0.575552	0.002210	0.716461
-11.827905	-1.943763	0.580557	0.002277	0.716164
-12.428623	-1.849256	0.585562	0.002389	0.716140
-12.222295	-1.882712	0.590566	0.002350	0.716147
-11.957326	-1.933983	0.595571	0.002301	0.716139
-12.316595	-1.868066	0.600576	0.002368	0.716144
-12.384297	-1.855269	0.605581	0.002380	0.716145
-12.059393	-1.928681	0.610586	0.002319	0.716115
-12.794626	-1.907469	0.615590	0.002456	0.715898
-13.267345	-1.826068	0.620595	0.002544	0.715893
-13.326424	-1.812484	0.625600	0.002554	0.715899
-12.786450	-1.908883	0.630605	0.002454	0.715899
-13.252474	-1.830840	0.635610	0.002540	0.715890
-13.271054	-1.824392	0.640614	0.002544	0.715897
-13.124508	-1.874810	0.645619	0.002516	0.715849
-13.956551	-1.873745	0.650624	0.002671	0.715557
-14.050726	-1.857178	0.655629	0.002688	0.715557
-14.291408	-1.818684	0.660634	0.002733	0.715549
-13.740390	-1.910833	0.665638	0.002630	0.715562
-13.987475	-1.871670	0.670643	0.002676	0.715552
-14.068027	-1.855364	0.675648	0.002690	0.715557
-13.852083	-1.920968	0.680653	0.002650	0.715503
-15.234886	-1.807978	0.685658	0.002907	0.715239
-15.103511	-1.827774	0.690662	0.002883	0.715247
-15.020018	-1.847894	0.695667	0.002867	0.715237
-14.971695	-1.854507	0.700672	0.002858	0.715241
-14.911717	-1.865873	0.705677	0.002846	0.715240
-15.249711	-1.808073	0.710682	0.002909	0.715236
-14.807598	-1.880826	0.715686	0.002826	0.715248
-15.373690	-1.891566	0.720691	0.002932	0.715027
-16.324635	-1.779907	0.725696	0.003108	0.714913
-15.506429	-1.922773	0.730701	0.002956	0.714919
-15.859541	-1.864519	0.735706	0.003021	0.714910
-15.981053	-1.838990	0.740710	0.003044	0.714918
-15.715458	-1.889347	0.745715	0.002994	0.714913
-15.967969	-1.842053	0.750720	0.003041	0.714918
-16.259980	-1.851274	0.755725	0.003095	0.714797
-16.939113	-1.823911	0.760730	0.003221	0.714611
-16.560101	-1.887790	0.765734	0.003151	0.714619
-17.116670	-1.793836	0.770739	0.003254	0.714609
-16.942117	-1.821840	0.775744	0.003221	0.714616
-16.367894	-1.924232	0.780749	0.003114	0.714616
-16.933291	-1.825521	0.785754	0.003219	0.714612
-16.739832	-1.899623	0.790758	0.003183	0.714534
-17.561522	-1.882190	0.795763	0.003336	0.714278
-17.639983	-1.867242	0.800768	0.003350	0.714281
-17.998268	-1.800750	0.805773	0.003417	0.714286
-18.151055	-1.777000	0.810778	0.003445	0.714280
-17.419866	-1.905080	0.815782	0.003308	0.714285
-17.843555	-1.833106	0.820787	0.003387	0.714278
-17.770939	-1.844562	0.825792	0.003373	0.714281
-17.980334	-1.940447	0.830797	0.003412	0.714017
-18.827806	-1.811702	0.835802	0.003570	0.713973
-18.768767	-1.817638	0.840806	0.003558	0.713983
-18.592682	-1.854128	0.845811	0.003525	0.713973
-18.801865	-1.816793	0.850816	0.003564	0.713974
-18.784322	-1.816868	0.855821	0.003561	0.713980
-18.898840	-1.803115	0.860826	0.003582	0.713967
-18.768625	-1.885352	0.865830	0.003557	0.713850
-19.791226	-1.802506	0.870835	0.003748	0.713653
-19.532321	-1.847352	0.875840	0.003699	0.713656
-19.425239	-1.863342	0.880845	0.003679	0.713663
-19.590887	-1.838042	0.885850	0.003710	0.713655
-19.567749	-1.838604	0.890854	0.003705	0.713662
-19.632918	-1.830814	0.895859	0.003717	0.713655
-19.572199	-1.872381	0.900864	0.003705	0.713594
-20.160376	-1.881298	0.905869	0.003815	0.713369
-20.598791	-1.806808	0.910874	0.003896	0.713362
-20.328902	-1.850669	0.915878	0.003846	0.713371
-20.307289	-1.857279	0.920883	0.003841	0.713366
-20.482365	-1.826452	0.925888	0.003874	0.713365
-20.515989	-1.820434	0.930893	0.003880	0.713366
-20.426373	-1.869335	0.935898	0.003863	0.713301
-21.666704	-1.783144	0.940902	0.004094	0.713033
-21.578940	-1.801892	0.945907	0.004077	0.713027
-21.470754	-1.819534	0.950912	0.004057	0.713031
-21.244310	-1.858403	0.955917	0.004014	0.713034
-21.545718	-1.810046	0.960922	0.004070	0.713024
-21.251417	-1.856495	0.965926	0.004015	0.713036
-21.287784	-1.854460	0.970931	0.004022	0.713028
-21.921795	-1.848328	0.975936	0.004140	0.712816
-22.306561	-1.827380	0.980941	0.004211	0.712721
-22.035043	-1.880437	0.985946	0.004160	0.712712
-22.275467	-1.833025	0.990950	0.004205	0.712722
-22.578192	-1.783528	0.995955	0.004261	0.712714
-22.218312	-1.845194	1.000960	0.004194	0.712719
-22.400092	-1.812465	1.005965	0.004227	0.712720
-22.585279	-1.841456	1.010970	0.004262	0.712597
-23.106731	-1.848804	1.015974	0.004359	0.712398
-23.012654	-1.869968	1.020979	0.004341	0.712389
-23.963957	-1.697850	1.025984	0.004518	0.712395
-23.536169	-1.774401	1.030989	0.004438	0.712395
-23.238135	-1.831946	1.035994	0.004382	0.712386
-23.469196	-1.785577	1.040998	0.004425	0.712397
-23.535806	-1.778854	1.046003	0.004437	0.712387
-23.262145	-1.916212	1.051008	0.004386	0.712211
-24.169830	-1.810307	1.056013	0.004555	0.712100
-24.476614	-1.759337	1.061018	0.004612	0.712093
-23.985922	-1.841575	1.066022	0.004520	0.712104
-24.447276	-1.765609	1.071027	0.004606	0.712092
-24.498284	-1.755162	1.076032	0.004615	0.712095
-24.161426	-1.812183	1.081037	0.004552	0.712102
-24.319463	-1.814585	1.086042	0.004581	0.712041
-25.183514	-1.794625	1.091046	0.004742	0.711774
-25.338141	-1.771861	1.096051	0.004771	0.711765
-25.546907	-1.733069	1.101056	0.004809	0.711769
-25.050455	-1.820254	1.106061	0.004717	0.711772
-25.370847	-1.767834	1.111066	0.004776	0.711763
-25.142644	-1.805145	1.116070	0.004733	0.711770
-25.095401	-1.815612	1.121075	0.004724	0.711766
-25.426375	-1.843584	1.126080	0.004786	0.711593
-26.182797	-1.773145	1.131085	0.004926	0.711466
-25.856497	-1.834707	1.136090	0.004865	0.711459
-26.010104	-1.803983	1.141094	0.004894	0.711466
-26.234456	-1.768440	1.146099	0.004935	0.711458
-25.686668	-1.866105	1.151104	0.004833	0.711458
-25.822832	-1.838529	1.156109	0.004858	0.711465
-26.506053	-1.812964	1.161114	0.004985	0.711274
-27.323505	-1.731889	1.166118	0.005137	0.711145
-26.794472	-1.828131	1.171123	0.005038	0.711142
-26.909184	-1.806803	1.176128	0.005060	0.711144
-27.155110	-1.761272	1.181133	0.005105	0.711148
-27.226449	-1.753462	1.186138	0.005118	0.711138
-26.977471	-1.793619	1.191142	0.005072	0.711147
-27.147553	-1.767665	1.196147	0.005103	0.711139
-27.423193	-1.847760	1.201152	0.005154	0.710881
-27.541487	-1.829312	1.206157	0.005176	0.710877
-27.941717	-1.763478	1.211162	0.005250	0.710866
-27.516645	-1.833023	1.216166	0.005171	0.710879
-27.860897	-1.775248	1.221171	0.005235	0.710872
-28.037832	-1.742950	1.226176	0.005267	0.710874
-27.626072	-1.841517	1.231181	0.005191	0.710824
-28.602912	-1.812733	1.236186	0.005372	0.710534
-28.289470	-1.864579	1.241190	0.005314	0.710543
-28.812828	-1.774687	1.246195	0.005411	0.710537
-28.859717	-1.767009	1.251200	0.005419	0.710536
-28.416593	-1.843450	1.256205	0.005337	0.710541
-28.840853	-1.772977	1.261210	0.005416	0.710531
-28.732696	-1.823720	1.266214	0.005395	0.710469
-29.396328	-1.830597	1.271219	0.005519	0.710219
-29.383390	-1.832057	1.276224	0.005516	0.710221
-29.716444	-1.770061	1.281229	0.005578	0.710227
-29.632730	-1.789876	1.286234	0.005562	0.710218
-29.135924	-1.874089	1.291238	0.005469	0.710227
-29.634808	-1.788322	1.296243	0.005562	0.710221
-29.855058	-1.791773	1.301248	0.005603	0.710136
-30.015804	-1.879891	1.306253	0.005632	0.709903
-30.153888	-1.860684	1.311258	0.005658	0.709893
-30.765659	-1.747104	1.316262	0.005771	0.709902
-30.462020	-1.803299	1.321267	0.005715	0.709898
-30.546822	-1.789059	1.326272	0.005730	0.709897
-30.667829	-1.765556	1.331277	0.005753	0.709901
-30.684676	-1.777363	1.336282	0.005756	0.709872
-30.917436	-1.868640	1.341286	0.005799	0.709607
-31.288468	-1.808265	1.346291	0.005868	0.709596
-31.556870	-1.758767	1.351296	0.005917	0.709600
-31.162051	-1.828052	1.356301	0.005844	0.709602
-31.437194	-1.781645	1.361306	0.005895	0.709597
-31.490089	-1.769462	1.366310	0.005904	0.709603
-31.474846	-1.774650	1.371315	0.005901	0.709599
-31.697386	-1.891176	1.376320	0.005942	0.709287
-32.330146	-1.784932	1.381325	0.006060	0.709274
-32.812938	-1.704714	1.386330	0.006150	0.709263
-31.986377	-1.847085	1.391334	0.005996	0.709273
-32.263374	-1.801672	1.396339	0.006047	0.709266
-32.363892	-1.783420	1.401344	0.006065	0.709267
-31.839775	-1.873918	1.406349	0.005968	0.709273
-32.653994	-1.869089	1.411354	0.006119	0.708993
-33.253894	-1.777001	1.416358	0.006230	0.708963
-33.044366	-1.818256	1.421363	0.006191	0.708956
-33.010003	-1.825136	1.426368	0.006185	0.708955
-32.981944	-1.827148	1.431373	0.006179	0.708961
-33.180596	-1.794487	1.436378	0.006216	0.708956
-32.798957	-1.865910	1.441382	0.006145	0.708950
-33.545200	-1.886414	1.446387	0.006283	0.708643
-33.939645	-1.818192	1.451392	0.006357	0.708639
-33.984513	-1.806897	1.456397	0.006365	0.708646
-33.953004	-1.817983	1.461402	0.006359	0.708636
-34.159861	-1.775362	1.466406	0.006397	0.708648
-34.049743	-1.798665	1.471411	0.006376	0.708641
-34.036100	-1.801539	1.476416	0.006373	0.708640
-34.526173	-1.851034	1.481421	0.006465	0.708366
-34.971697	-1.781379	1.486426	0.006547	0.708347
-34.737022	-1.818741	1.491430	0.006503	0.708357
-34.765295	-1.816325	1.496435	0.006508	0.708352
-35.024971	-1.771926	1.501440	0.006557	0.708349
-34.717074	-1.823585	1.506445	0.006499	0.708355
-34.610676	-1.853781	1.511450	0.006479	0.708333
-35.818492	-1.796386	1.516454	0.006704	0.708017
-35.858001	-1.790993	1.521459	0.006711	0.708014
-35.905262	-1.783012	1.526464	0.006719	0.708014
-35.541828	-1.843950	1.531469	0.006651	0.708022
-35.894658	-1.785748	1.536474	0.006717	0.708013
-35.786761	-1.802269	1.541478	0.006697	0.708019
-35.617791	-1.835320	1.546483	0.006665	0.708013
-36.263011	-1.845356	1.551488	0.006785	0.707763
-36.629508	-1.807131	1.556493	0.006853	0.707709
-36.621924	-1.810910	1.561498	0.006851	0.707705
-36.596952	-1.811484	1.566502	0.006846	0.707713
-37.043164	-1.735895	1.571507	0.006929	0.707705
-36.937085	-1.755284	1.576512	0.006909	0.707705
-36.622834	-1.809015	1.581517	0.006851	0.707710
-36.766812	-1.850526	1.586522	0.006877	0.707576
-37.478165	-1.818081	1.591526	0.007009	0.707387
-37.144615	-1.879610	1.596531	0.006947	0.707383
-37.952533	-1.734489	1.601536	0.007097	0.707386
-37.825161	-1.754523	1.606541	0.007073	0.707391
-37.571970	-1.805386	1.611546	0.007026	0.707380
-37.688500	-1.782918	1.616550	0.007047	0.707384
-37.667676	-1.828648	1.621555	0.007043	0.707300
-38.409471	-1.801622	1.626560	0.007181	0.707089
-38.103121	-1.853094	1.631565	0.007124	0.707096
-38.977863	-1.702552	1.636570	0.007287	0.707086
-38.376818	-1.805309	1.641574	0.007175	0.707095
-38.345845	-1.813760	1.646579	0.007169	0.707090
-38.824725	-1.729504	1.651584	0.007257	0.707088
-38.557566	-1.787830	1.656589	0.007208	0.707067
-39.102338	-1.846638	1.661594	0.007309	0.706754
-39.180511	-1.829571	1.666598	0.007323	0.706761
-39.336185	-1.803429	1.671603	0.007352	0.706758
-39.308183	-1.811466	1.676608	0.007346	0.706752
-39.215083	-1.823064	1.681613	0.007329	0.706763
-39.532716	-1.772288	1.686618	0.007388	0.706751
-39.172475	-1.868885	1.691622	0.007321	0.706687
-39.932165	-1.851930	1.696627	0.007462	0.706449
-40.465048	-1.757615	1.701632	0.007561	0.706448
-40.187003	-1.804824	1.706637	0.007509	0.706453
-39.990696	-1.846901	1.711642	0.007472	0.706440
-39.946882	-1.849793	1.716646	0.007464	0.706450
-40.265201	-1.794852	1.721651	0.007523	0.706447
-40.346206	-1.824703	1.726656	0.007538	0.706358
-40.968311	-1.823982	1.731661	0.007653	0.706137
-41.225263	-1.783240	1.736666	0.007701	0.706127
-41.143544	-1.794483	1.741670	0.007685	0.706134
-40.919089	-1.835752	1.746675	0.007643	0.706132
-41.249588	-1.779492	1.751680	0.007705	0.706127
-40.904668	-1.836333	1.756685	0.007640	0.706137
-40.973460	-1.859102	1.761690	0.007653	0.706067
-41.618548	-1.843214	1.766694	0.007773	0.705868
-41.546034	-1.858290	1.771699	0.007759	0.705864
-41.833623	-1.807931	1.776704	0.007812	0.705863
-41.330654	-1.894037	1.781709	0.007718	0.705871
-41.726271	-1.825972	1.786714	0.007792	0.705866
-41.707289	-1.829953	1.791718	0.007788	0.705865
-42.341279	-1.884093	1.796723	0.007906	0.705529
-42.844386	-1.795040	1.801728	0.007999	0.705528
-42.849144	-1.791376	1.806733	0.008000	0.705535
-42.537353	-1.852636	1.811738	0.007942	0.705524
-42.691287	-1.821021	1.816742	0.007970	0.705532
-42.849576	-1.795106	1.821747	0.007999	0.705528
-42.563291	-1.864309	1.826752	0.007946	0.705492
-43.162860	-1.893087	1.831757	0.008057	0.705219
-43.717912	-1.797448	1.836762	0.008161	0.705213
-43.936975	-1.756472	1.841766	0.008201	0.705217
-43.415565	-1.850409	1.846771	0.008104	0.705216
-43.700726	-1.802069	1.851776	0.008157	0.705211
-43.752606	-1.788609	1.856781	0.008166	0.705220
-43.528169	-1.835110	1.861786	0.008124	0.705208
-44.385403	-1.839323	1.866790	0.008284	0.704892
-44.842587	-1.755974	1.871795	0.008368	0.704896
-44.712666	-1.782328	1.876800	0.008344	0.704890
-44.164704	-1.876932	1.881805	0.008242	0.704897
-44.935111	-1.742431	1.886810	0.008385	0.704891
-44.674733	-1.786308	1.891814	0.008336	0.704897
-44.275172	-1.859454	1.896819	0.008262	0.704893
-45.093117	-1.812412	1.901824	0.008414	0.704695
-45.942849	-1.707036	1.906829	0.008572	0.704602
-45.686594	-1.757423	1.911834	0.008524	0.704593
-45.419211	-1.804100	1.916838	0.008474	0.704596
-45.712554	-1.751431	1.921843	0.008528	0.704597
-45.467461	-1.795878	1.926848	0.008482	0.704596
-45.400008	-1.803851	1.931853	0.008470	0.704604
-45.544810	-1.796179	1.936858	0.008496	0.704568
-46.111550	-1.843586	1.941862	0.008602	0.704269
-46.031177	-1.859363	1.946867	0.008586	0.704267
-46.369989	-1.800871	1.951872	0.008649	0.704263
-46.210399	-1.826822	1.956877	0.008619	0.704269
-46.300487	-1.815190	1.961882	0.008636	0.704260
-46.142144	-1.839602	1.966886	0.008606	0.704269
-46.155010	-1.902516	1.971891	0.008608	0.704137
-47.371751	-1.776517	1.976896	0.008835	0.703955
-46.624033	-1.906900	1.981901	0.008695	0.703961
-47.065385	-1.832330	1.986906	0.008777	0.703953
-47.201592	-1.803650	1.991910	0.008802	0.703962
-46.922367	-1.853254	1.996915	0.008750	0.703963
-47.279468	-1.839218	2.001920	0.008817	0.703863

-48.163342	-1.792291	2.011917	0.008981	0.703641
-48.134882	-1.799409	2.021914	0.008975	0.703638
-47.957762	-1.830012	2.031910	0.008941	0.703640
-48.165367	-1.793028	2.041907	0.008980	0.703641
-48.093898	-1.808124	2.051904	0.008966	0.703637
-47.990257	-1.826787	2.061901	0.008946	0.703638
-47.956425	-1.833276	2.071898	0.008940	0.703638
-47.963441	-1.830777	2.081894	0.008940	0.703641
-48.202739	-1.788491	2.091891	0.008984	0.703641
-47.947173	-1.794967	2.101888	0.008936	0.703721
-47.312792	-1.792964	2.111885	0.008818	0.703954
-47.417794	-1.774622	2.121882	0.008837	0.703954
-47.184354	-1.814683	2.131878	0.008793	0.703958
-47.397661	-1.776877	2.141875	0.008832	0.703958
-47.154057	-1.821462	2.151872	0.008787	0.703957
-47.225251	-1.764198	2.161869	0.008799	0.704048
-46.514314	-1.784313	2.171866	0.008667	0.704263
-46.348657	-1.813257	2.181862	0.008635	0.704266
-46.263671	-1.827702	2.191859	0.008619	0.704268
-46.137156	-1.851838	2.201856	0.008595	0.704265
-46.019409	-1.750378	2.211853	0.008573	0.704513
-45.680412	-1.770821	2.221850	0.008509	0.704595
-45.482515	-1.806869	2.231846	0.008472	0.704594
-45.666662	-1.773487	2.241843	0.008506	0.704596
-44.879666	-1.779446	2.251840	0.008359	0.704867
-44.750448	-1.790755	2.261837	0.008334	0.704892
-44.532654	-1.829263	2.271834	0.008293	0.704893
-44.584362	-1.815068	2.281830	0.008302	0.704904
-44.004673	-1.762693	2.291827	0.008194	0.705218
-43.552403	-1.844242	2.301824	0.008109	0.705217
-43.930207	-1.777191	2.311821	0.008179	0.705218
-43.545162	-1.807351	2.321818	0.008107	0.705296
-42.844878	-1.816152	2.331814	0.007976	0.705530
-42.982422	-1.790186	2.341811	0.008002	0.705534
-42.912950	-1.803376	2.351808	0.007988	0.705533
-42.332993	-1.785634	2.361805	0.007880	0.705778
-41.994967	-1.802131	2.371802	0.007816	0.705867
-41.923563	-1.813762	2.381798	0.007803	0.705870
-41.942507	-1.807966	2.391795	0.007806	0.705875
-41.600859	-1.740875	2.401792	0.007742	0.706134
-41.165406	-1.819927	2.411789	0.007660	0.706132
-41.275466	-1.800959	2.421786	0.007680	0.706131
-40.816660	-1.767808	2.431782	0.007594	0.706363
-40.325908	-1.812733	2.441779	0.007503	0.706449
-40.196626	-1.835535	2.451776	0.007478	0.706451
-40.442673	-1.762184	2.461773	0.007523	0.706511
-39.590831	-1.792723	2.471770	0.007364	0.706755
-39.476751	-1.812814	2.481766	0.007343	0.706757
-39.692970	-1.773640	2.491763	0.007382	0.706759
-38.970552	-1.751907	2.501760	0.007248	0.707062
-38.651403	-1.796756	2.511757	0.007188	0.707087
-38.566796	-1.811631	2.521754	0.007172	0.707088
-38.551041	-1.740380	2.531750	0.007168	0.707238
-37.614026	-1.835893	2.541747	0.006993	0.707382
-37.811577	-1.801760	2.551744	0.007030	0.707381
-38.123948	-1.729207	2.561741	0.007087	0.707415
-36.946702	-1.796379	2.571738	0.006868	0.707702
-36.906724	-1.802442	2.581734	0.006860	0.707705
-36.749258	-1.829562	2.591731	0.006830	0.707708
-36.533074	-1.777286	2.601728	0.006789	0.707891
-36.007053	-1.809134	2.611725	0.006691	0.708016
-36.152669	-1.784104	2.621722	0.006718	0.708015
-36.105679	-1.766272	2.631718	0.006708	0.708068
-35.199876	-1.784018	2.641715	0.006539	0.708357
-35.278997	-1.769514	2.651712	0.006554	0.708359
-35.217114	-1.783184	2.661709	0.006542	0.708354
-34.822149	-1.750122	2.671706	0.006468	0.708563
-34.590655	-1.749545	2.681702	0.006424	0.708647
-34.449507	-1.775314	2.691699	0.006397	0.708647
-34.071525	-1.771806	2.701696	0.006327	0.708790
-33.447848	-1.798448	2.711693	0.006210	0.708960
-33.655819	-1.761604	2.721690	0.006248	0.708960
-33.470814	-1.794916	2.731686	0.006213	0.708960
-32.789476	-1.770114	2.741683	0.006086	0.709254
-32.885388	-1.745276	2.751680	0.006104	0.709270
-32.553579	-1.807797	2.761677	0.006041	0.709264
-32.168189	-1.787884	2.771674	0.005969	0.709442
-31.677864	-1.796886	2.781670	0.005877	0.709600
-31.715897	-1.787790	2.791667	0.005884	0.709605
-31.690881	-1.794541	2.801664	0.005879	0.709602
-31.168469	-1.756672	2.811661	0.005781	0.709864
-30.891777	-1.789826	2.821658	0.005729	0.709897
-30.757792	-1.813183	2.831654	0.005704	0.709899
-30.628189	-1.765820	2.841651	0.005679	0.710041
-29.857680	-1.812987	2.851648	0.005535	0.710222
-29.965286	-1.794345	2.861645	0.005555	0.710222
-29.877987	-1.811298	2.871642	0.005538	0.710220
-29.261049	-1.793632	2.881638	0.005423	0.710476
-29.056931	-1.799711	2.891635	0.005385	0.710537
-29.179932	-1.777504	2.901632	0.005407	0.710538
-28.969439	-1.768869	2.911629	0.005367	0.710631
-28.046836	-1.810603	2.921626	0.005195	0.710877
-27.803581	-1.853860	2.931622	0.005150	0.710878
-28.039791	-1.811323	2.941619	0.005193	0.710880
-27.813662	-1.778903	2.951616	0.005151	0.711026
-27.169605	-1.832846	2.961613	0.005030	0.711148
-27.432246	-1.787950	2.971610	0.005079	0.711145
-27.343678	-1.781239	2.981606	0.005062	0.711191
-26.647574	-1.769654	2.991603	0.004932	0.711462
-26.430098	-1.809294	3.001600	0.004891	0.711461
-26.370361	-1.821062	3.011597	0.004879	0.711460
-25.727892	-1.828866	3.021594	0.004759	0.711673
-25.478493	-1.825631	3.031590	0.004712	0.711769
-25.713962	-1.783424	3.041587	0.004756	0.711771
-25.556869	-1.779454	3.051584	0.004726	0.711835
-24.890400	-1.769042	3.061581	0.004601	0.712093
-24.880255	-1.769894	3.071578	0.004599	0.712096
-24.781310	-1.787001	3.081574	0.004580	0.712098
-24.011719	-1.784005	3.091571	0.004436	0.712378
-23.737239	-1.825051	3.101568	0.004385	0.712395
-23.945019	-1.789897	3.111565	0.004423	0.712392
-23.925267	-1.720184	3.121562	0.004419	0.712538
-22.842934	-1.824948	3.131558	0.004217	0.712715
-23.243802	-1.753626	3.141555	0.004291	0.712715
-22.885085	-1.802846	3.151552	0.004224	0.712745
-22.031933	-1.812712	3.161549	0.004065	0.713029
-22.226328	-1.779122	3.171546	0.004101	0.713028
-21.971098	-1.824779	3.181542	0.004053	0.713028
-21.784942	-1.767597	3.191539	0.004017	0.713209
-21.274875	-1.780244	3.201536	0.003922	0.713365
-21.401962	-1.758372	3.211533	0.003945	0.713365
-21.223818	-1.777917	3.221530	0.003912	0.713390
-20.386698	-1.792057	3.231526	0.003755	0.713659
-20.306941	-1.806331	3.241523	0.003740	0.713660
-20.240329	-1.818577	3.251520	0.003727	0.713660
-20.146343	-1.742844	3.261517	0.003709	0.713845
-19.449156	-1.800156	3.271514	0.003579	0.713978
-19.435956	-1.802138	3.281510	0.003576	0.713980
-19.656319	-1.748233	3.291507	0.003617	0.714010
-18.664419	-1.786711	3.301504	0.003432	0.714285
-18.568900	-1.803320	3.311501	0.003413	0.714287
-18.646245	-1.790784	3.321498	0.003427	0.714285
-18.216986	-1.768399	3.331494	0.003347	0.714482
-17.556638	-1.817662	3.341491	0.003224	0.714619
-17.663513	-1.798803	3.351488	0.003243	0.714620
-17.625613	-1.807153	3.361485	0.003236	0.714617
-17.070614	-1.768334	3.371482	0.003132	0.714891
-16.958189	-1.776258	3.381478	0.003110	0.714916
-16.869532	-1.792233	3.391475	0.003094	0.714917
-16.402257	-1.786610	3.401472	0.003006	0.715094
-16.015895	-1.782347	3.411469	0.002934	0.715240
-16.055808	-1.775496	3.421466	0.002941	0.715240
-15.799960	-1.821334	3.431462	0.002893	0.715240
-15.156880	-1.783689	3.441459	0.002772	0.715543
-14.707522	-1.858401	3.451456	0.002688	0.715554
-14.950019	-1.816999	3.461453	0.002733	0.715552
-14.771749	-1.826429	3.471450	0.002699	0.715597
-14.134545	-1.791243	3.481446	0.002580	0.715892
-13.988141	-1.816754	3.491443	0.002553	0.715894
-13.808422	-1.850133	3.501440	0.002519	0.715892
-13.969620	-1.766422	3.511437	0.002548	0.716002
-12.999304	-1.870696	3.521434	0.002367	0.716139
-13.312102	-1.814762	3.531430	0.002425	0.716140
-13.454124	-1.776663	3.541427	0.002451	0.716166
-12.487396	-1.802495	3.551424	0.002271	0.716457
-12.335208	-1.831521	3.561421	0.002242	0.716454
-12.027451	-1.886799	3.571418	0.002184	0.716454
-12.034476	-1.810492	3.581414	0.002185	0.716603
-11.124541	-1.891978	3.591411	0.002015	0.716764
-11.352044	-1.852186	3.601408	0.002057	0.716763
-11.503811	-1.825688	3.611405	0.002085	0.716763
-10.704599	-1.828457	3.621402	0.001936	0.717040
-10.560518	-1.826965	3.631398	0.001908	0.717094
-10.281431	-1.877884	3.641395	0.001856	0.717093
-10.291542	-1.850188	3.651392	0.001857	0.717145
-9.470386	-1.873383	3.661389	0.001704	0.717389
-9.396604	-1.887614	3.671386	0.001690	0.717388
-9.732548	-1.827600	3.681382	0.001752	0.717389
-9.193426	-1.845781	3.691379	0.001651	0.717544
-8.673578	-1.854618	3.701376	0.001554	0.717710
-8.828625	-1.829515	3.711373	0.001582	0.717706
-8.659163	-1.854105	3.721370	0.001550	0.717718
-8.234154	-1.777004	3.731366	0.001471	0.718021
-7.610389	-1.887849	3.741363	0.001354	0.718022
-7.944002	-1.828371	3.751360	0.001416	0.718023
-7.378279	-1.825611	3.761357	0.001310	0.718228
-6.910014	-1.843854	3.771354	0.001223	0.718358
-7.137309	-1.801572	3.781350	0.001264	0.718362
-6.678757	-1.879940	3.791347	0.001179	0.718369
-6.450696	-1.779530	3.801344	0.001136	0.718649
-6.085591	-1.846082	3.811341	0.001067	0.718646
-6.379862	-1.793415	3.821338	0.001122	0.718648
-5.669085	-1.799597	3.831334	0.000989	0.718886
-5.223860	-1.838311	3.841331	0.000906	0.718967
-5.443663	-1.801601	3.851328	0.000946	0.718963
-5.032554	-1.832134	3.861325	0.000869	0.719048
-4.410228	-1.828314	3.871322	0.000753	0.719275
-4.269295	-1.854465	3.881318	0.000726	0.719274
-4.277972	-1.851633	3.891315	0.000727	0.719277
-3.943098	-1.789284	3.901312	0.000664	0.719519
-3.299120	-1.859189	3.911309	0.000544	0.719608
-3.492163	-1.826654	3.921306	0.000580	0.719605
-3.344026	-1.828829	3.931302	0.000552	0.719653
-2.730154	-1.810387	3.941299	0.000437	0.719906
-2.902458	-1.780594	3.951296	0.000468	0.719905
-2.550896	-1.844652	3.961293	0.000403	0.719903
-2.460323	-1.728008	3.971290	0.000385	0.720165
-2.058748	-1.768152	3.981286	0.000310	0.720228
-1.896025	-1.796396	3.991283	0.000279	0.720230
-1.939541	-1.679790	4.001280	0.000287	0.720445
-1.539494	-1.700748	4.011277	0.000212	0.720545
-1.857243	-1.644938	4.021274	0.000271	0.720544
-1.629127	-1.520611	4.031270	0.000228	0.720870
-1.209367	-1.586999	4.041267	0.000149	0.720887
-1.664196	-1.440316	4.051264	0.000233	0.721017
-1.143148	-1.477613	4.061261	0.000136	0.721127
-1.106815	-1.421789	4.071258	0.000129	0.721250
-1.026428	-1.337863	4.081254	0.000113	0.721444
-0.904907	-1.297101	4.091251	0.000090	0.721568
-0.813911	-1.221145	4.101248	0.000073	0.721750
-0.518990	-1.192138	4.111245	0.000017	0.721911
-0.548467	-1.101768	4.121242	0.000022	0.722079
-0.521732	-1.003397	4.131238	0.000017	0.722282
-0.566910	-0.936023	4.141235	0.000025	0.722399
-0.609883	-0.777369	4.151232	0.000032	0.722697
-0.743333	-0.658912	4.161229	0.000057	0.722883
-0.536450	-0.590868	4.171226	0.000018	0.723090
-0.135497	-0.532792	4.181222	-0.000058	0.723345
0.037227	-0.438859	4.191219	-0.000090	0.723590
-0.112983	-0.309963	4.201216	-0.000063	0.723791
-0.147510	-0.188948	4.211213	-0.000057	0.724017
-0.085540	-0.073103	4.221210	-0.000069	0.724266
-0.210610	0.120164	4.231206	-0.000046	0.724601
0.000000	0.224702	4.241203	-0.000086	0.724880

0.252417	0.809821	4.246208	-0.000134	0.726112
0.266720	2.076058	4.251213	-0.000137	0.728587
0.709066	3.870458	4.256218	-0.000221	0.732224
1.072947	6.222908	4.261222	-0.000291	0.736891
1.277910	9.123388	4.266227	-0.000331	0.742522
1.643542	12.474406	4.271232	-0.000401	0.749018
2.395011	16.210817	4.276237	-0.000544	0.756310
3.504283	20.301037	4.281242	-0.000753	0.764307
4.337862	24.849145	4.286246	-0.000912	0.772971
5.921947	29.648255	4.291251	-0.001210	0.782235
7.427679	34.833746	4.296256	-0.001494	0.792057
8.464687	40.420828	4.301261	-0.001691	0.802321
9.426869	46.340850	4.306266	-0.001874	0.813013
10.043580	52.577268	4.311270	-0.001993	0.824005
11.165896	59.022519	4.316275	-0.002207	0.835358
12.486980	65.633589	4.321280	-0.002457	0.846895
13.459366	72.545590	4.326285	-0.002643	0.858671
14.289812	79.697400	4.331290	-0.002802	0.870638
14.972022	87.041610	4.336294	-0.002934	0.882708
16.096345	94.505923	4.341299	-0.003149	0.894929
16.989559	102.156235	4.346304	-0.003320	0.907212
17.601983	109.998291	4.351309	-0.003440	0.919550
18.405302	117.921785	4.356314	-0.003595	0.931899
18.826538	126.017937	4.361318	-0.003679	0.944245
19.317001	134.213332	4.366323	-0.003776	0.956596
20.041512	142.436926	4.371328	-0.003916	0.968890
20.581519	150.766990	4.376333	-0.004022	0.981138
21.513002	159.144305	4.381338	-0.004201	0.993398
22.042639	167.592909	4.386342	-0.004306	1.005511
22.795992	176.061290	4.391347	-0.004452	1.017561
23.156883	184.629485	4.396352	-0.004525	1.029513
23.716765	193.183862	4.401357	-0.004635	1.041355
24.178565	201.796070	4.406362	-0.004727	1.053120
24.676972	210.401409	4.411366	-0.004825	1.064753
25.015092	219.085672	4.416371	-0.004894	1.076327
25.852003	227.649091	4.421376	-0.005056	1.087733
26.685679	236.246392	4.426381	-0.005217	1.099063
27.332418	244.894514	4.431386	-0.005343	1.110301
27.577131	253.588262	4.436390	-0.005394	1.121396
28.057604	262.249079	4.441395	-0.005490	1.132392
28.516964	270.900500	4.446400	-0.005581	1.143266
28.846360	279.603715	4.451405	-0.005648	1.154073
29.520337	288.193493	4.456410	-0.005780	1.164713
30.047769	296.797536	4.461414	-0.005884	1.175244
30.564381	305.397082	4.466419	-0.005986	1.185674
30.880773	314.031763	4.471424	-0.006050	1.196013
31.291677	322.611738	4.476429	-0.006133	1.206218
31.897579	331.179532	4.481434	-0.006251	1.216362
32.002147	339.791190	4.486438	-0.006277	1.226374
33.076286	348.268918	4.491443	-0.006482	1.236340
34.050115	356.716792	4.496448	-0.006670	1.246172
34.463624	365.271184	4.501453	-0.006752	1.255940
34.902116	373.803058	4.506458	-0.006840	1.265612
35.265681	382.336094	4.511462	-0.006913	1.275197
35.553928	390.845135	4.516467	-0.006973	1.284671
35.980019	399.335643	4.521472	-0.007058	1.294080
36.815758	407.729797	4.526477	-0.007219	1.303391
37.954791	416.186805	4.531482	-0.007437	1.312758
38.329593	424.668878	4.536486	-0.007512	1.321949
38.705064	433.110376	4.541491	-0.007588	1.331032
39.208556	441.521171	4.546496	-0.007687	1.340044
39.443476	449.951352	4.551501	-0.007737	1.348968
39.616033	458.405700	4.556506	-0.007775	1.357849
40.210805	466.735517	4.561510	-0.007891	1.366615
40.482290	475.154841	4.566515	-0.007947	1.375362
40.804906	483.529207	4.571520	-0.008013	1.384016
41.175357	491.908743	4.576525	-0.008088	1.392630
42.023128	500.184938	4.581530	-0.008251	1.401166
42.326895	508.536374	4.586534	-0.008314	1.409635
42.995989	516.842681	4.591539	-0.008444	1.418068
44.016662	525.069250	4.596544	-0.008639	1.426430
44.405509	533.433570	4.601549	-0.008717	1.434776
44.885948	541.755964	4.606554	-0.008813	1.443047
45.390246	550.062639	4.611558	-0.008912	1.451260
45.909045	558.378732	4.616563	-0.009014	1.459437
46.107407	566.729201	4.621568	-0.009057	1.467551
46.470688	575.085051	4.626573	-0.009130	1.475651
47.116888	583.321030	4.631578	-0.009256	1.483637
47.389483	591.622651	4.636582	-0.009313	1.491584
47.920499	599.879498	4.641587	-0.009417	1.499486
48.519555	608.121050	4.646592	-0.009534	1.507343
48.675465	616.436076	4.651597	-0.009569	1.515160
49.027526	624.703142	4.656602	-0.009640	1.522922
49.544081	632.928799	4.661606	-0.009742	1.530631
50.064005	641.176079	4.666611	-0.009844	1.538321
50.412583	649.425991	4.671616	-0.009915	1.545950
50.448207	657.754825	4.676621	-0.009927	1.553567
51.049682	665.944499	4.681626	-0.010044	1.561104
51.332751	674.190707	4.686630	-0.010103	1.568609
51.591023	682.442419	4.691635	-0.010156	1.576079
51.815627	690.684097	4.696640	-0.010204	1.583500
52.082196	698.914872	4.701645	-0.010259	1.590883
52.615902	707.111002	4.706650	-0.010364	1.598239
52.961575	715.308508	4.711654	-0.010434	1.605536
53.751374	723.473776	4.716659	-0.010587	1.612833
54.042772	731.700021	4.721664	-0.010646	1.620081
54.299752	739.925945	4.726669	-0.010700	1.627292
54.904653	748.166802	4.731674	-0.010818	1.634532
54.977751	756.382481	4.736678	-0.010837	1.641644
55.399625	764.559437	4.741683	-0.010921	1.648741
55.956979	772.732135	4.746688	-0.011031	1.655822
56.501550	780.872665	4.751693	-0.011138	1.662843
56.772084	789.099663	4.756698	-0.011193	1.669871
56.939125	797.316517	4.761702	-0.011230	1.676847
57.506648	805.463736	4.766707	-0.011341	1.683789
57.794690	813.666508	4.771712	-0.011401	1.690711
57.996627	821.864452	4.776717	-0.011444	1.697590
58.345786	830.047684	4.781722	-0.011514	1.704448
58.816613	838.222283	4.786726	-0.011608	1.711287
59.235643	846.397733	4.791731	-0.011691	1.718093
59.582609	854.554270	4.796736	-0.011761	1.724847
59.981339	862.711946	4.801741	-0.011841	1.731582
60.392046	870.887112	4.806746	-0.011923	1.738307
60.857453	879.010410	4.811750	-0.012015	1.744970
61.691538	887.121895	4.816755	-0.012176	1.751645
62.172688	895.287170	4.821760	-0.012271	1.758294
62.476654	903.436591	4.826765	-0.012333	1.764882
63.159210	911.586918	4.831770	-0.012466	1.771493
63.190384	919.808005	4.836774	-0.012477	1.778056
63.399328	927.987832	4.841779	-0.012522	1.784583
63.997732	936.142535	4.846784	-0.012639	1.791114
64.285084	944.325293	4.851789	-0.012698	1.797606
64.501249	952.477751	4.856794	-0.012744	1.804041
64.652087	960.628938	4.861798	-0.012777	1.810445
65.316876	968.727999	4.866803	-0.012906	1.816848
65.662910	976.868255	4.871808	-0.012976	1.823221
65.960466	985.013551	4.876813	-0.013037	1.829571
66.584519	993.142090	4.881818	-0.013159	1.835924
66.760941	1001.285082	4.886822	-0.013197	1.842213
67.406586	1009.378603	4.891827	-0.013323	1.848498
67.916840	1017.514291	4.896832	-0.013424	1.854778
68.203507	1025.653164	4.901837	-0.013483	1.861013
68.531746	1033.814094	4.906842	-0.013549	1.867249
68.892202	1041.967347	4.911846	-0.013622	1.873461
69.315553	1050.087442	4.916851	-0.013706	1.879635
69.787052	1058.195291	4.921856	-0.013799	1.885786
69.887302	1066.355627	4.926861	-0.013824	1.891913
70.396960	1074.470949	4.931866	-0.013924	1.898033
71.026406	1082.546063	4.936870	-0.014047	1.904117
71.094459	1090.741667	4.941875	-0.014065	1.910207
71.617922	1098.855327	4.946880	-0.014168	1.916269
71.933691	1106.967390	4.951885	-0.014232	1.922287
72.374915	1115.091353	4.956890	-0.014320	1.928308
72.656111	1123.232591	4.961894	-0.014378	1.934306
73.237858	1131.303432	4.966899	-0.014492	1.940267
73.636303	1139.424800	4.971904	-0.014571	1.946226
73.733627	1147.621997	4.976909	-0.014595	1.952189
74.054343	1155.746315	4.981914	-0.014660	1.958106
74.336296	1163.824841	4.986918	-0.014718	1.963967
74.665618	1171.923072	4.991923	-0.014785	1.969830
74.988439	1180.050623	4.996928	-0.014851	1.975696
75.322942	1188.122641	5.001933	-0.014918	1.981506
75.589232	1196.250727	5.006938	-0.014974	1.987331
75.738527	1204.397441	5.011942	-0.015007	1.993140
76.142687	1212.474445	5.016947	-0.015088	1.998910
76.665441	1220.543846	5.021952	-0.015190	2.004670
77.191146	1228.625161	5.026957	-0.015294	2.010422
77.476333	1236.767649	5.031962	-0.015352	2.016176
77.777880	1244.861654	5.036966	-0.015414	2.021881
77.976406	1252.993982	5.041971	-0.015456	2.027585
78.539124	1261.108756	5.046976	-0.015567	2.033299
78.833296	1269.189855	5.051981	-0.015627	2.038946
79.091405	1277.297334	5.056986	-0.015681	2.044592
79.401279	1285.394525	5.061990	-0.015744	2.050220
80.031588	1293.455266	5.066995	-0.015867	2.055841
80.545898	1301.532364	5.072000	-0.015968	2.061445
80.674365	1309.658612	5.077005	-0.015997	2.067029
80.932689	1317.794406	5.082010	-0.016051	2.072617
81.505321	1325.848119	5.087014	-0.016163	2.078165
81.825520	1333.944471	5.092019	-0.016228	2.083703
81.995779	1342.078201	5.097024	-0.016265	2.089236
82.631531	1350.135117	5.102029	-0.016389	2.094748
83.018589	1358.242402	5.107034	-0.016467	2.100256
83.080089	1366.364053	5.112038	-0.016484	2.105727
83.318208	1374.518392	5.117043	-0.016534	2.111222
83.662363	1382.638011	5.122048	-0.016603	2.116691
83.971751	1390.679273	5.127053	-0.016666	2.122089
84.133574	1398.788796	5.132058	-0.016702	2.127505
84.622198	1406.843434	5.137062	-0.016798	2.132902
85.014434	1414.912177	5.142067	-0.016877	2.138286
85.204491	1423.012581	5.147072	-0.016918	2.143657
85.675100	1431.060576	5.152077	-0.017011	2.149007
86.228077	1439.151683	5.157082	-0.017119	2.154380
86.534445	1447.223100	5.162086	-0.017182	2.159703
86.745806	1455.299798	5.167091	-0.017227	2.165008
87.229875	1463.396437	5.172096	-0.017322	2.170338
87.400472	1471.497201	5.177101	-0.017360	2.175628
87.915650	1479.556864	5.182106	-0.017461	2.180910
88.233536	1487.636461	5.187110	-0.017526	2.186175
88.588702	1495.749848	5.192115	-0.017597	2.191452
89.226234	1503.822296	5.197120	-0.017721	2.196715
89.269851	1511.912937	5.202125	-0.017735	2.201924
89.572661	1519.990371	5.207130	-0.017797	2.207135
89.748943	1528.106170	5.212134	-0.017835	2.212347
89.992349	1536.189238	5.217139	-0.017886	2.217532
90.633797	1544.220557	5.222144	-0.018011	2.222708
90.866739	1552.295418	5.227149	-0.018060	2.227862
90.880923	1560.456755	5.232154	-0.018068	2.233040
91.147510	1568.514832	5.237158	-0.018123	2.238163
91.951208	1576.498253	5.242163	-0.018278	2.243274
92.147052	1584.612772	5.247168	-0.018320	2.248403
92.389803	1592.716316	5.252173	-0.018371	2.253517
92.984810	1600.758318	5.257178	-0.018487	2.258612
93.295481	1608.840909	5.262182	-0.018550	2.263695
93.529521	1616.931500	5.267187	-0.018599	2.268766
94.018510	1625.074323	5.272192	-0.018696	2.273880
94.229411	1633.112331	5.277197	-0.018741	2.278893
94.639722	1641.157299	5.282202	-0.018823	2.283916
95.000511	1649.217257	5.287206	-0.018895	2.288934
95.261255	1657.301850	5.292211	-0.018949	2.293947
95.607454	1665.372531	5.297216	-0.019019	2.298947
95.723955	1673.440452	5.302221	-0.019046	2.303916
96.347033	1681.493635	5.307226	-0.019168	2.308907
96.589931	1689.602179	5.312230	-0.019219	2.313890
96.612662	1697.677612	5.317235	-0.019228	2.318823
97.022479	1705.727176	5.322240	-0.019310	2.323762
97.229227	1713.796911	5.327245	-0.019354	2.328686
97.509978	1721.898788	5.332250	-0.019412	2.333625
97.666584	1729.968322	5.337254	-0.019447	2.338524
98.111909	1738.000193	5.342259	-0.019535	2.343414
98.441576	1746.074675	5.347264	-0.019602	2.348309
98.524918	1754.191006	5.352269	-0.019623	2.353200
99.127979	1762.199926	5.357274	-0.019741	2.358057
99.324162	1770.267904	5.362278	-0.019783	2.362908
99.619941	1778.324025	5.367283	-0.019843	2.367749
100.007854	1786.413514	5.372288	-0.019921	2.372607
100.204646	1794.479672	5.377293	-0.019963	2.377427
100.638100	1802.527435	5.382298	-0.020049	2.382244
100.681475	1810.606895	5.387302	-0.020063	2.387039
101.327817	1818.641258	5.392307	-0.020188	2.391846
101.503319	1826.751939	5.397312	-0.020227	2.396651
101.715601	1834.786385	5.402317	-0.020272	2.401404
102.116902	1842.847316	5.407322	-0.020352	2.406178
102.580853	1850.902096	5.412326	-0.020444	2.410944
102.891934	1858.976365	5.417331	-0.020507	2.415700
103.238007	1867.039946	5.422336	-0.020577	2.420443
103.726332	1875.074782	5.427341	-0.020673	2.425171
103.858610	1883.193884	5.432346	-0.020703	2.429911
104.242376	1891.324765	5.437350	-0.020780	2.434668
104.606239	1899.326068	5.442355	-0.020854	2.439339
104.850127	1907.368724	5.447360	-0.020905	2.444016
105.245504	1915.389746	5.452365	-0.020984	2.448683
105.607897	1923.470474	5.457370	-0.021057	2.453372
105.941348	1931.512091	5.462374	-0.021124	2.458028
106.079943	1939.581351	5.467379	-0.021155	2.462677
106.508983	1947.640272	5.472384	-0.021241	2.467332
106.809698	1955.708243	5.477389	-0.021302	2.471974
107.229135	1963.771198	5.482394	-0.021386	2.476613
107.637197	1971.798165	5.487398	-0.021467	2.481223
107.769412	1979.878888	5.492403	-0.021497	2.485833
108.312887	1987.941184	5.497408	-0.021604	2.490455
108.507590	1996.024299	5.502413	-0.021646	2.495055
108.863889	2004.091089	5.507418	-0.021718	2.499648
108.884110	2012.144448	5.512422	-0.021727	2.504201
109.443084	2020.176295	5.517427	-0.021836	2.508773
109.693454	2028.305594	5.522432	-0.021888	2.513369
109.746497	2036.367712	5.527437	-0.021904	2.517904
110.233747	2044.363647	5.532442	-0.022000	2.522425
110.290284	2052.426898	5.537446	-0.022016	2.526945
110.493523	2060.481398	5.542451	-0.022059	2.531463
110.818799	2068.549397	5.547456	-0.022125	2.535988
111.068689	2076.572352	5.552461	-0.022177	2.540475
111.451557	2084.608180	5.557466	-0.022254	2.544971
111.755769	2092.680002	5.562470	-0.022316	2.549473
111.936653	2100.747822	5.567475	-0.022355	2.553956
112.217732	2108.804531	5.572480	-0.022413	2.558432
112.622149	2116.817765	5.577485	-0.022494	2.562884
112.727491	2124.907633	5.582490	-0.022519	2.567351
112.957214	2132.966729	5.587494	-0.022567	2.571801
113.148093	2141.034585	5.592499	-0.022608	2.576246
113.486409	2149.078016	5.597504	-0.022677	2.580679
113.669459	2157.125874	5.602509	-0.022716	2.585097
113.889421	2165.200434	5.607514	-0.022763	2.589524
114.076148	2173.447779	5.612518	-0.022803	2.594036
114.491136	2181.415980	5.617523	-0.022886	2.598403
114.824073	2189.416990	5.622528	-0.022953	2.602776
115.031118	2197.420861	5.627533	-0.022997	2.607133
115.455513	2205.451882	5.632538	-0.023082	2.611513
115.476850	2213.534569	5.637542	-0.023091	2.615887
115.763912	2221.543756	5.642547	-0.023150	2.620231
116.268543	2229.555132	5.647552	-0.023249	2.624583
116.437187	2237.609741	5.652557	-0.023286	2.628929
116.608545	2245.708275	5.657562	-0.023324	2.633292
117.016071	2253.723685	5.662566	-0.023405	2.637619
117.232311	2261.746278	5.667571	-0.023451	2.641929
117.494787	2269.811206	5.672576	-0.023505	2.646258
117.731202	2277.844407	5.677581	-0.023554	2.650562
118.084373	2285.914338	5.682586	-0.023626	2.654885
118.186102	2293.977572	5.687590	-0.023650	2.659182
118.506603	2302.002514	5.692595	-0.023715	2.663465
118.887727	2310.057344	5.697600	-0.023792	2.667761
119.062083	2318.122804	5.702605	-0.023830	2.672043
119.465004	2326.196609	5.707610	-0.023910	2.676336
119.822221	2334.206871	5.712614	-0.023982	2.680587
120.058240	2342.225758	5.717619	-0.024031	2.684827
120.267520	2350.294555	5.722624	-0.024076	2.689085
120.527296	2358.360067	5.727629	-0.024130	2.693338
120.757787	2366.412820	5.732634	-0.024178	2.697575
120.801954	2374.469756	5.737638	-0.024192	2.701797
120.821459	2382.510610	5.742643	-0.024201	2.706001
121.236165	2390.555525	5.747648	-0.024284	2.710226
121.457062	2398.625047	5.752653	-0.024330	2.714445
121.594474	2406.665594	5.757658	-0.024361	2.718638
121.972810	2414.674863	5.762662	-0.024437	2.722822
122.252649	2422.704193	5.767667	-0.024495	2.727004
122.449943	2430.780568	5.772672	-0.024537	2.731199
122.544210	2438.857545	5.777677	-0.024560	2.735382
122.799851	2446.880622	5.782682	-0.024613	2.739540
122.940359	2454.927241	5.787686	-0.024645	2.743697
123.123800	2462.971977	5.792691	-0.024684	2.747849
123.588289	2471.052385	5.797696	-0.024776	2.752031
123.702911	2479.137232	5.802701	-0.024803	2.756187
124.028450	2487.122374	5.807706	-0.024869	2.760298
124.413881	2495.110754	5.812710	-0.024946	2.764408
124.571731	2503.169099	5.817715	-0.024981	2.768535
124.651661	2511.255415	5.822720	-0.025001	2.772665
124.707336	2519.295334	5.827725	-0.025017	2.776763
125.215331	2527.288920	5.832730	-0.025117	2.780859
125.404384	2535.320625	5.837734	-0.025158	2.784949
125.614504	2543.381520	5.842739	-0.025203	2.789049
125.769834	2551.467546	5.847744	-0.025237	2.793153
125.821624	2559.502159	5.852749	-0.025252	2.797218
125.991139	2567.532417	5.857754	-0.025289	2.801282
126.432222	2575.548680	5.862758	-0.025377	2.805349
126.603818	2583.590497	5.867763	-0.025414	2.809408
126.813704	2591.680664	5.872768	-0.025459	2.813487
127.055929	2599.696823	5.877773	-0.025509	2.817524
127.521166	2607.717141	5.882778	-0.025601	2.821571
127.701151	2615.780005	5.887782	-0.025640	2.825617
127.992618	2623.806792	5.892787	-0.025700	2.829645
128.216183	2631.911150	5.897792	-0.025747	2.833703
128.385100	2639.925019	5.902797	-0.025784	2.837706
128.726186	2647.933254	5.907802	-0.025853	2.841710
128.782681	2655.997210	5.912806	-0.025869	2.845721
128.984396	2663.989400	5.917811	-0.025912	2.849698
129.306754	2672.082632	5.922816	-0.025977	2.853727
129.245871	2680.134140	5.927821	-0.025972	2.857708
129.442728	2688.155801	5.932826	-0.026014	2.861683
129.736580	2696.189851	5.937830	-0.026074	2.865664
129.711797	2704.238046	5.942835	-0.026075	2.869628
130.071673	2712.312030	5.947840	-0.026147	2.873621
130.324160	2720.315372	5.952845	-0.026200	2.877568
130.615115	2728.338919	5.957850	-0.026259	2.881522
130.807622	2736.375703	5.962854	-0.026301	2.885471
131.367452	2744.372513	5.967859	-0.026410	2.889415
131.357155	2752.507191	5.972864	-0.026414	2.893390
131.455903	2760.531500	5.977869	-0.026438	2.897311
131.733456	2768.555278	5.982874	-0.026495	2.901237
132.031371	2776.577562	5.987878	-0.026556	2.905157
131.968004	2784.653923	5.992883	-0.026549	2.909080
132.520910	2792.757606	5.997888	-0.026658	2.913043
132.562223	2800.799325	6.002893	-0.026671	2.916943
132.694764	2808.801814	6.007898	-0.026701	2.920824
132.923907	2816.797981	6.012902	-0.026749	2.924702
133.111839	2824.798398	6.017907	-0.026790	2.928574
133.500234	2832.867976	6.022912	-0.026867	2.932486
133.663518	2840.923114	6.027917	-0.026903	2.936373
133.747692	2848.964491	6.032922	-0.026924	2.940244
134.047477	2856.984004	6.037926	-0.026986	2.944111
134.047376	2865.005038	6.042931	-0.026991	2.947958
134.555464	2873.035719	6.047936	-0.027091	2.951831
134.754081	2881.085825	6.052941	-0.027134	2.955692
135.033605	2889.096650	6.057946	-0.027191	2.959533
135.047524	2897.161676	6.062950	-0.027199	2.963381
135.183046	2905.180869	6.067955	-0.027230	2.967209
135.588713	2913.229462	6.072960	-0.027311	2.971060
135.659835	2921.283762	6.077965	-0.027330	2.974891
135.834678	2929.299893	6.082970	-0.027368	2.978705
136.374870	2937.319739	6.087974	-0.027474	2.982534
136.715493	2945.333146	6.092979	-0.027542	2.986344
137.044994	2953.383928	6.097984	-0.027609	2.990167
137.343125	2961.471678	6.102989	-0.027670	2.994001
137.489205	2969.490656	6.107994	-0.027703	2.997790
137.606660	2977.529520	6.112998	-0.027730	3.001582
137.752010	2985.536493	6.118003	-0.027763	3.005356
138.129748	2993.555754	6.123008	-0.027839	3.009142
138.304021	3001.629999	6.128013	-0.027876	3.012939
138.551484	3009.672854	6.133018	-0.027928	3.016720
138.918748	3017.709393	6.138022	-0.028002	3.020499
139.084516	3025.683678	6.143027	-0.028038	3.024234
139.312680	3033.761116	6.148032	-0.028086	3.028016
139.536732	3041.812358	6.153037	-0.028133	3.031781
139.648782	3049.883354	6.158042	-0.028160	3.035545
139.685815	3057.882878	6.163046	-0.028172	3.039267
139.894019	3065.903439	6.168051	-0.028216	3.043003
140.276027	3073.934197	6.173056	-0.028293	3.046747
140.281551	3081.994980	6.178061	-0.028299	3.050483
140.516830	3090.034586	6.183066	-0.028348	3.054215
140.766787	3098.053586	6.188070	-0.028400	3.057934
140.963649	3106.081161	6.193075	-0.028443	3.061649
141.233575	3114.117217	6.198080	-0.028498	3.065367
141.369828	3122.136809	6.203085	-0.028529	3.069067
141.542400	3130.248024	6.208090	-0.028567	3.072806
141.727514	3138.308785	6.213094	-0.028607	3.076519
142.042977	3146.268797	6.218099	-0.028671	3.080186
142.283792	3154.291014	6.223104	-0.028721	3.083874
142.158747	3162.339502	6.228109	-0.028703	3.087553
142.563233	3170.366617	6.233114	-0.028784	3.091242
142.787800	3178.427821	6.238118	-0.028831	3.094933
143.072875	3186.405711	6.243123	-0.028890	3.098585
143.354239	3194.455933	6.248128	-0.028948	3.102266
143.485485	3202.484225	6.253133	-0.028978	3.105925
143.626606	3210.527945	6.258138	-0.029009	3.109588
143.843038	3218.592979	6.263142	-0.029055	3.113259
143.943982	3226.599926	6.268147	-0.029079	3.116894
144.336742	3234.642451	6.273152	-0.029158	3.120554
144.530618	3242.636325	6.278157	-0.029199	3.124179
144.537760	3250.680200	6.283162	-0.029206	3.127814
144.768831	3258.761844	6.288166	-0.029255	3.131472
144.924018	3266.772538	6.293171	-0.029289	3.135090
145.274528	3274.794159	6.298176	-0.029360	3.138718
145.284441	3282.821196	6.303181	-0.029367	3.142328
145.601074	3290.854527	6.308186	-0.029432	3.145951
145.794411	3298.886374	6.313190	-0.029473	3.149563
145.938613	3306.944195	6.318195	-0.029505	3.153181
146.219963	3314.998682	6.323200	-0.029563	3.156799
146.281376	3322.986147	6.328205	-0.029580	3.160374
146.264661	3331.019650	6.333210	-0.029582	3.163961
146.577376	3339.027557	6.338214	-0.029646	3.167547
147.098004	3347.037922	6.343219	-0.029748	3.171140
147.226494	3355.127753	6.348224	-0.029778	3.174746
147.265163	3363.161031	6.353229	-0.029790	3.178320
147.550778	3371.160656	6.358234	-0.029849	3.181885
147.803473	3379.216922	6.363238	-0.029902	3.185469
147.926332	3387.231376	6.368243	-0.029930	3.189026
148.297038	3395.268578	6.373248	-0.030004	3.192599
148.450675	3403.329307	6.378253	-0.030038	3.196169
148.517676	3411.329567	6.383258	-0.030056	3.199705
148.785497	3419.334526	6.388262	-0.030112	3.203248
148.934998	3427.371745	6.393267	-0.030145	3.206796
149.047296	3435.424303	6.398272	-0.030171	3.210345
149.322968	3443.469001	6.403277	-0.030228	3.213893
149.588045	3451.498127	6.408282	-0.030283	3.217430
149.712098	3459.564428	6.413286	-0.030312	3.220974
149.697465	3467.515821	6.418291	-0.030314	3.224458
150.032602	3475.580814	6.423296	-0.030382	3.228002
150.510257	3483.612248	6.428301	-0.030476	3.231533
150.802210	3491.680024	6.433306	-0.030536	3.235069
150.869190	3499.686050	6.438310	-0.030554	3.238565
151.245765	3507.678493	6.443315	-0.030630	3.242063
151.441955	3515.725881	6.448320	-0.030672	3.245575
151.489794	3523.740484	6.453325	-0.030686	3.249062
151.701613	3531.787440	6.458330	-0.030731	3.252566
152.008313	3539.829418	6.463334	-0.030794	3.256068
152.070518	3547.777987	6.468339	-0.030811	3.259516
152.530839	3555.844261	6.473344	-0.030902	3.263027
152.617603	3563.901607	6.478349	-0.030923	3.266515
152.644314	3571.938393	6.483354	-0.030934	3.269989
153.151062	3579.981302	6.488358	-0.031034	3.273480
153.336812	3587.994830	6.493363	-0.031074	3.276943
153.473653	3596.030066	6.498368	-0.031105	3.280409
153.628795	3604.038822	6.503373	-0.031139	3.283860
153.837933	3612.039584	6.508378	-0.031183	3.287307
153.915326	3620.124743	6.513382	-0.031203	3.290781
153.760343	3628.159982	6.518387	-0.031180	3.294221
154.041685	3636.197970	6.523392	-0.031238	3.297676
154.391986	3644.189459	6.528397	-0.031308	3.301109
154.679244	3652.198726	6.533402	-0.031367	3.304545
154.929903	3660.248989	6.538406	-0.031419	3.307992
155.160946	3668.305131	6.543411	-0.031468	3.311438
155.189017	3676.368727	6.548416	-0.031479	3.314876
155.493032	3684.350996	6.553421	-0.031541	3.318285
155.719643	3692.355809	6.558426	-0.031588	3.321698
155.854345	3700.410888	6.563430	-0.031619	3.325126
155.930798	3708.401458	6.568435	-0.031638	3.328520
156.142747	3716.452438	6.573440	-0.031683	3.331941
156.629411	3724.484810	6.578445	-0.031779	3.335362
156.559978	3732.494498	6.583450	-0.031772	3.338748
156.778824	3740.539643	6.588454	-0.031818	3.342157
156.997654	3748.529496	6.593459	-0.031864	3.345538
157.075047	3756.603498	6.598464	-0.031884	3.348947
157.530580	3764.653044	6.603469	-0.031974	3.352356
157.911384	3772.672197	6.608474	-0.032051	3.355745
158.300981	3780.671408	6.613478	-0.032129	3.359123
158.246810	3788.684293	6.618483	-0.032124	3.362487
158.760282	3796.692227	6.623488	-0.032225	3.365867
158.781738	3804.755777	6.628493	-0.032235	3.369248
159.109283	3812.785653	6.633498	-0.032301	3.372623
159.108027	3820.878617	6.638502	-0.032306	3.376009
159.259335	3828.822522	6.643507	-0.032340	3.379335
159.717221	3836.862036	6.648512	-0.032431	3.382708
159.723792	3844.919525	6.653517	-0.032437	3.386070
159.731587	3852.922719	6.658522	-0.032444	3.389405
160.107588	3861.026596	6.663526	-0.032520	3.392792
160.158038	3869.081242	6.668531	-0.032535	3.396144
160.342251	3877.047716	6.673536	-0.032574	3.399461
160.696580	3885.022136	6.678541	-0.032646	3.402783
160.638960	3893.066007	6.683546	-0.032640	3.406117
161.001338	3901.046591	6.688550	-0.032713	3.409435
161.232549	3909.084511	6.693555	-0.032762	3.412770
161.470688	3917.175164	6.698560	-0.032812	3.416123
161.828604	3925.131650	6.703565	-0.032884	3.419422
161.927936	3933.172573	6.708570	-0.032908	3.422744
162.278199	3941.227238	6.713574	-0.032978	3.426076
162.365570	3949.215930	6.718579	-0.033000	3.429369
162.477954	3957.311269	6.723584	-0.033026	3.432704
162.738969	3965.333251	6.728589	-0.033080	3.436010
162.796621	3973.324893	6.733594	-0.033097	3.439294
163.042477	3981.359158	6.738598	-0.033148	3.442598
163.118374	3989.373895	6.743603	-0.033167	3.445885
163.272004	3997.428943	6.748608	-0.033202	3.449189
163.132832	4005.505497	6.753613	-0.033181	3.452488
163.396597	4013.516772	6.758618	-0.033236	3.455771
163.698781	4021.516645	6.763622	-0.033297	3.459047
163.763207	4029.526453	6.768627	-0.033315	3.462317
164.187164	4037.514367	6.773632	-0.033399	3.465586
164.278424	4045.597163	6.778637	-0.033422	3.468879
164.438543	4053.624620	6.783642	-0.033457	3.472150
164.506748	4061.703914	6.788646	-0.033475	3.475435
164.685811	4069.648246	6.793651	-0.033514	3.478666
164.847225	4077.661515	6.798656	-0.033549	3.481921
164.956787	4085.694928	6.803661	-0.033575	3.485180
164.951522	4093.705590	6.808666	-0.033580	3.488423
165.284386	4101.761311	6.813670	-0.033647	3.491692
165.400987	4109.782128	6.818675	-0.033674	3.494936
165.676924	4117.784882	6.823680	-0.033731	3.498176
165.889072	4125.835000	6.828685	-0.033776	3.501429
165.932333	4133.810470	6.833690	-0.033789	3.504644
166.368197	4141.873081	6.838694	-0.033876	3.507903
166.403569	4149.912965	6.843699	-0.033888	3.511138
166.872330	4157.914477	6.848704	-0.033981	3.514368
166.817388	4165.952906	6.853709	-0.033976	3.517593
167.163614	4173.952384	6.858714	-0.034046	3.520812
167.440173	4181.942069	6.863718	-0.034103	3.524022
167.512811	4190.004649	6.868723	-0.034122	3.527252
167.692950	4198.053212	6.873728	-0.034161	3.530477
167.856892	4206.096383	6.878733	-0.034197	3.533696
168.079780	4214.139383	6.883738	-0.034244	3.536914
168.219342	4222.175745	6.888742	-0.034275	3.540124
168.400022	4230.170919	6.893747	-0.034314	3.543315
168.669716	4238.202012	6.898752	-0.034370	3.546521
168.800180	4246.251711	6.903757	-0.034400	3.549727
168.728263	4254.345870	6.908762	-0.034392	3.552942
169.149013	4262.400421	6.913766	-0.034476	3.556152
169.216899	4270.331192	6.918771	-0.034494	3.559301
169.392792	4278.313032	6.923776	-0.034532	3.562469
169.542421	4286.332400	6.928781	-0.034565	3.565650
169.615570	4294.361483	6.933786	-0.034584	3.568828
169.871917	4302.407214	6.938790	-0.034637	3.572016
170.013786	4310.409334	6.943795	-0.034669	3.575181
170.235661	4318.397726	6.948800	-0.034716	3.578339
170.651597	4326.450440	6.953805	-0.034799	3.581526
170.715973	4334.410796	6.958810	-0.034816	3.584663
171.011328	4342.490781	6.963814	-0.034877	3.587851
171.183678	4350.493253	6.968819	-0.034914	3.591003
171.135527	4358.529878	6.973824	-0.034911	3.594158
171.326515	4366.588975	6.978829	-0.034952	3.597327
171.529883	4374.569159	6.983834	-0.034995	3.600462
171.945916	4382.579446	6.988838	-0.035078	3.603612
171.955122	4390.621180	6.993843	-0.035085	3.606760
172.181160	4398.651328	6.998848	-0.035133	3.609907
171.835167	4406.745973	7.003853	-0.035074	3.613061
172.222661	4414.736432	7.008858	-0.035151	3.616191
172.605978	4422.699861	7.013862	-0.035228	3.619308
172.555359	4430.745755	7.018867	-0.035224	3.622443
172.752394	4438.753949	7.023872	-0.035266	3.625567
172.781969	4446.821809	7.028877	-0.035277	3.628707
172.934375	4454.871231	7.033882	-0.035311	3.631840
173.102379	4462.929008	7.038886	-0.035348	3.634974
173.448163	4470.889728	7.043891	-0.035418	3.638073
173.847786	4478.910059	7.048896	-0.035498	3.641193
173.942357	4486.907718	7.053901	-0.035521	3.644294
174.063287	4494.949158	7.058906	-0.035549	3.647410
174.280414	4502.987703	7.063910	-0.035595	3.650524
174.447786	4510.997823	7.068915	-0.035631	3.653624
174.591839	4519.038262	7.073920	-0.035663	3.656732
174.744543	4527.062354	7.078925	-0.035697	3.659831
174.978067	4535.038404	7.083930	-0.035746	3.662911
175.387694	4543.119673	7.088934	-0.035828	3.666034
175.427700	4551.126616	7.093939	-0.035841	3.669115
175.934509	4559.163350	7.098944	-0.035941	3.672218
176.041210	4567.190854	7.103949	-0.035966	3.675304
176.207892	4575.177201	7.108954	-0.036002	3.678373
176.299029	4583.227467	7.113958	-0.036025	3.681462
176.589209	4591.195495	7.118963	-0.036084	3.684523
176.854162	4599.260072	7.123968	-0.036139	3.687617
177.022570	4607.299550	7.128973	-0.036176	3.690696
177.207806	4615.329187	7.133978	-0.036216	3.693769
177.392285	4623.346839	7.138982	-0.036256	3.696835
177.381380	4631.325912	7.143987	-0.036259	3.699879
177.673521	4639.347478	7.148992	-0.036319	3.702944
177.770831	4647.415576	7.153997	-0.036342	3.706020
177.946442	4655.395888	7.159002	-0.036381	3.709061
178.089544	4663.490896	7.164006	-0.036413	3.712143
178.313547	4671.537336	7.169011	-0.036460	3.715206
178.542131	4679.498905	7.174016	-0.036508	3.718234
178.697595	4687.527754	7.179021	-0.036542	3.721283
178.662297	4695.474104	7.184026	-0.036541	3.724294
179.153976	4703.548327	7.189030	-0.036638	3.727363
179.101966	4711.579797	7.194035	-0.036634	3.730401
179.364742	4719.607764	7.199040	-0.036688	3.733443
179.521884	4727.632538	7.204045	-0.036723	3.736478
179.795372	4735.612731	7.209050	-0.036779	3.739496
180.099790	4743.648074	7.214054	-0.036841	3.742534
180.437937	4751.646535	7.219059	-0.036910	3.745556
180.354462	4759.711930	7.224064	-0.036900	3.748591
180.622851	4767.745342	7.229069	-0.036955	3.751620
180.912370	4775.730056	7.234074	-0.037015	3.754628
181.148399	4783.791137	7.239078	-0.037064	3.757661
181.113545	4791.823938	7.244083	-0.037063	3.760675
181.270395	4799.782274	7.249088	-0.037098	3.763664
181.395583	4807.909819	7.254093	-0.037126	3.766712
181.312095	4815.881565	7.259098	-0.037116	3.769695
181.663986	4823.939134	7.264102	-0.037187	3.772717
181.932823	4831.953219	7.269107	-0.037243	3.775719
182.294715	4839.903793	7.274112	-0.037316	3.778697
182.498507	4847.995025	7.279117	-0.037359	3.781721
182.618380	4855.930362	7.284122	-0.037387	3.784683
182.963738	4864.024440	7.289126	-0.037456	3.787706
183.014951	4872.047904	7.294131	-0.037471	3.790695
183.156790	4880.077376	7.299136	-0.037503	3.793685
183.391508	4888.146397	7.304141	-0.037552	3.796690
183.298171	4896.042857	7.309146	-0.037540	3.799621
183.459778	4904.135699	7.314150	-0.037576	3.802628
183.654177	4912.084874	7.319155	-0.037618	3.805580
184.051637	4920.143061	7.324160	-0.037697	3.808574
184.087624	4928.186672	7.329165	-0.037709	3.811554
184.051425	4936.188456	7.334170	-0.037708	3.814513
184.334054	4944.232894	7.339174	-0.037766	3.817493
184.445148	4952.251375	7.344179	-0.037792	3.820457
184.599936	4960.215240	7.349184	-0.037826	3.823400
184.786967	4968.296941	7.354189	-0.037867	3.826385
184.880018	4976.276000	7.359194	-0.037889	3.829327
185.029282	4984.328439	7.364198	-0.037923	3.832296
185.413102	4992.328046	7.369203	-0.038000	3.835247
185.425254	5000.325280	7.374208	-0.038007	3.838188
185.649863	5008.374492	7.379213	-0.038055	3.841150
185.730387	5016.336022	7.384218	-0.038075	3.844074
186.229275	5024.397736	7.389222	-0.038173	3.847042
186.141623	5032.436413	7.394227	-0.038163	3.849986
186.224281	5040.506710	7.399232	-0.038183	3.852944
186.561205	5048.547833	7.404237	-0.038252	3.855893
186.788222	5056.492867	7.409242	-0.038299	3.858803
186.874382	5064.554316	7.414246	-0.038321	3.861751
186.932074	5072.553389	7.419251	-0.038337	3.864673
187.170054	5080.614615	7.424256	-0.038387	3.867619
187.416014	5088.619127	7.429261	-0.038438	3.870542
187.507111	5096.845675	7.434266	-0.038460	3.873541
187.872100	5104.862219	7.439270	-0.038534	3.876466
187.675906	5112.752051	7.444275	-0.038503	3.879332
187.785933	5120.716283	7.449280	-0.038529	3.882229
188.063925	5128.711938	7.454285	-0.038586	3.885138
188.295446	5136.702420	7.459290	-0.038634	3.888043
188.522725	5144.756048	7.464294	-0.038682	3.890968
188.519948	5152.785771	7.469299	-0.038687	3.893877
188.899046	5160.813471	7.474304	-0.038763	3.896791
189.137922	5168.813275	7.479309	-0.038813	3.899690
189.101185	5176.830095	7.484314	-0.038812	3.902588
189.357048	5184.830710	7.489318	-0.038865	3.905484
189.345490	5192.869423	7.494323	-0.038868	3.908386
189.485399	5200.900223	7.499328	-0.038900	3.911285
189.802838	5208.950435	7.504333	-0.038964	3.914193
190.024651	5216.952723	7.509338	-0.039011	3.917080
190.235283	5224.938160	7.514342	-0.039055	3.919958
190.249072	5232.965635	7.519347	-0.039063	3.922845
190.462811	5240.954138	7.524352	-0.039109	3.925720
190.912321	5248.987991	7.529357	-0.039198	3.928614
190.782141	5257.029294	7.534362	-0.039179	3.931497
191.082241	5265.078395	7.539366	-0.039240	3.934389
191.238343	5273.085838	7.544371	-0.039275	3.937262
191.317794	5281.076850	7.549376	-0.039295	3.940124
191.498010	5289.114981	7.554381	-0.039334	3.943004
191.599655	5297.112290	7.559386	-0.039359	3.945865
191.897464	5305.160879	7.564390	-0.039419	3.948746
191.938193	5313.174709	7.569395	-0.039432	3.951608
192.166323	5321.209745	7.574400	-0.039480	3.954479
192.551330	5329.225583	7.579405	-0.039558	3.957343
192.344681	5337.205894	7.584410	-0.039524	3.960183
192.830614	5345.237433	7.589414	-0.039620	3.963050
192.802513	5353.264556	7.594419	-0.039621	3.965905
192.900480	5361.223784	7.599424	-0.039644	3.968736
193.184734	5369.267796	7.604429	-0.039703	3.971599
193.391942	5377.292357	7.609434	-0.039747	3.974451
193.662134	5385.353262	7.614438	-0.039802	3.977314
193.627995	5393.342773	7.619443	-0.039802	3.980146
193.777711	5401.367271	7.624448	-0.039835	3.982990
193.997852	5409.409295	7.629453	-0.039881	3.985841
194.048397	5417.406772	7.634458	-0.039896	3.988670
194.136792	5425.492152	7.639462	-0.039918	3.991529
194.740311	5433.488029	7.644467	-0.040036	3.994363
194.584166	5441.518484	7.649472	-0.040012	3.997195
194.743963	5449.544578	7.654477	-0.040047	4.000028
194.808202	5457.514319	7.659482	-0.040065	4.002838
194.888734	5465.533297	7.664486	-0.040085	4.005663
194.907597	5473.589156	7.669491	-0.040094	4.008498
195.146485	5481.619546	7.674496	-0.040144	4.011326
195.378335	5489.665801	7.679501	-0.040193	4.014158
195.436065	5497.687349	7.684506	-0.040209	4.016976
195.528173	5505.655193	7.689510	-0.040232	4.019773
195.713711	5513.692195	7.694515	-0.040272	4.022595
195.803406	5521.682990	7.699520	-0.040294	4.025396
195.880166	5529.769144	7.704525	-0.040313	4.028229
196.307070	5537.761010	7.709530	-0.040398	4.031032
196.502271	5545.874048	7.714534	-0.040440	4.033873
196.572141	5553.874073	7.719539	-0.040459	4.036669
196.692870	5561.797009	7.724544	-0.040487	4.039438
197.032377	5569.807373	7.729549	-0.040555	4.042238
196.927361	5577.792202	7.734554	-0.040541	4.045021
196.699820	5585.865652	7.739558	-0.040504	4.047831
197.268819	5593.862616	7.744563	-0.040616	4.050625
197.428284	5601.889711	7.749568	-0.040651	4.053420
197.501053	5609.948495	7.754573	-0.040670	4.056224
197.560841	5617.865149	7.759578	-0.040686	4.058976
197.980969	5625.947662	7.764582	-0.040770	4.061789
198.127599	5633.922134	7.769587	-0.040803	4.064558
198.316769	5641.961608	7.774592	-0.040843	4.067349
198.524720	5649.983395	7.779597	-0.040888	4.070132
198.616598	5658.028105	7.784602	-0.040910	4.072919
198.878424	5666.035408	7.789606	-0.040964	4.075694
198.972275	5673.995439	7.794611	-0.040987	4.078449
199.270283	5682.035863	7.799616	-0.041048	4.081231
199.492357	5690.046047	7.804621	-0.041095	4.084001
199.642473	5698.068241	7.809626	-0.041128	4.086772
199.834482	5706.075281	7.814630	-0.041169	4.089536
199.840320	5714.151311	7.819635	-0.041176	4.092320
199.700864	5722.174144	7.824640	-0.041156	4.095081
199.998677	5730.188077	7.829645	-0.041216	4.097843
200.090302	5738.196451	7.834650	-0.041239	4.100599
200.280626	5746.194651	7.839654	-0.041280	4.103351
200.447898	5754.229192	7.844659	-0.041316	4.106113
200.661726	5762.271087	7.849664	-0.041362	4.108876
200.903048	5770.301974	7.854669	-0.041412	4.111634
201.183493	5778.337799	7.859674	-0.041470	4.114392
201.400767	5786.353246	7.864678	-0.041516	4.117141
201.562926	5794.336975	7.869683	-0.041551	4.119876
201.693603	5802.355551	7.874688	-0.041581	4.122621
201.929010	5810.384804	7.879693	-0.041630	4.125369
201.917868	5818.375547	7.884698	-0.041634	4.128099
202.268424	5826.462655	7.889702	-0.041704	4.130864
202.073344	5834.490940	7.894707	-0.041674	4.133601
202.300045	5842.500077	7.899712	-0.041721	4.136335
202.463146	5850.483903	7.904717	-0.041757	4.139057
202.667849	5858.498171	7.909722	-0.041801	4.141789
202.892855	5866.512512	7.914726	-0.041848	4.144519
203.185683	5874.565658	7.919731	-0.041908	4.147261
203.230563	5882.561295	7.924736	-0.041922	4.149978
203.556572	5890.640656	7.929741	-0.041988	4.152726
203.500034	5898.652307	7.934746	-0.041983	4.155444
203.661213	5906.623909	7.939750	-0.042018	4.158150
203.800157	5914.638398	7.944755	-0.042049	4.160868
203.871290	5922.610721	7.949760	-0.042068	4.163569
204.174286	5930.670796	7.954765	-0.042130	4.166301
204.313566	5938.671659	7.959770	-0.042161	4.169009
204.357765	5946.741958	7.964774	-0.042175	4.171737
204.575605	5954.745206	7.969779	-0.042221	4.174444
204.588682	5962.740193	7.974784	-0.042229	4.177143
204.780295	5970.766869	7.979789	-0.042270	4.179853
204.710686	5978.770362	7.984794	-0.042263	4.182551
205.034809	5986.744840	7.989798	-0.042328	4.185241
205.079866	5994.839371	7.994803	-0.042342	4.187967
205.205326	6002.814105	7.999808	-0.042371	4.190652
205.569214	6010.954466	8.004813	-0.042444	4.193394
205.618896	6018.962558	8.009818	-0.042459	4.196086
206.170604	6026.847419	8.014822	-0.042567	4.198740
206.186360	6034.930217	8.019827	-0.042575	4.201453
206.177200	6042.848645	8.024832	-0.042579	4.204109
206.562042	6050.937796	8.029837	-0.042656	4.206824
206.478472	6058.888309	8.034842	-0.042646	4.209486
206.701397	6066.965964	8.039846	-0.042693	4.212193
206.849799	6075.017580	8.044851	-0.042726	4.214888
206.820857	6082.974237	8.049856	-0.042726	4.217548
207.065129	6090.978165	8.054861	-0.042777	4.220225
207.143701	6099.010941	8.059866	-0.042797	4.222908
207.398859	6107.010865	8.064870	-0.042850	4.225580
207.860326	6115.049210	8.069875	-0.042942	4.228265
208.183895	6123.039742	8.074880	-0.043007	4.230932
208.415574	6131.153464	8.079885	-0.043056	4.233636
208.698332	6139.142456	8.084890	-0.043114	4.236298
208.867831	6147.132337	8.089894	-0.043151	4.238957
209.056703	6155.163399	8.094899	-0.043192	4.241629
209.247711	6163.115883	8.099904	-0.043233	4.244272
209.635474	6171.171347	8.104909	-0.043310	4.246951
209.594191	6179.165926	8.109914	-0.043308	4.249603
209.800408	6187.249039	8.114918	-0.043352	4.252285
210.047665	6195.253283	8.119923	-0.043403	4.254939
209.983390	6203.290017	8.124928	-0.043397	4.257600
210.168785	6211.281572	8.129933	-0.043437	4.260247
210.339150	6219.263476	8.134938	-0.043474	4.262888
210.515257	6227.288992	8.139942	-0.043512	4.265543
210.514719	6235.371553	8.144947	-0.043517	4.268213
210.594183	6243.373823	8.149952	-0.043538	4.270855
211.080083	6251.422507	8.154957	-0.043634	4.273515
211.127502	6259.426242	8.159962	-0.043648	4.276154
211.194865	6267.420218	8.164966	-0.043666	4.278789
211.302040	6275.469348	8.169971	-0.043691	4.281440
211.281830	6283.378721	8.174976	-0.043693	4.284043
211.351792	6291.498576	8.179981	-0.043711	4.286714
211.647739	6299.454456	8.184986	-0.043772	4.289332
211.787148	6307.538048	8.189990	-0.043803	4.291988
212.180651	6315.540544	8.194995	-0.043882	4.294619
212.331887	6323.583543	8.200000	-0.043916	4.297258
212.488532	6331.585707	8.205005	-0.043950	4.299883
212.461868	6339.580086	8.210010	-0.043951	4.302503
212.447780	6347.581894	8.215014	-0.043954	4.305123
212.563527	6355.629402	8.220019	-0.043981	4.307758
212.599818	6363.638880	8.225024	-0.043993	4.310378
212.657238	6371.696710	8.230029	-0.044009	4.313012
212.894717	6379.665480	8.235034	-0.044059	4.315617
212.990303	6387.679721	8.240038	-0.044082	4.318234
213.170098	6395.729503	8.245043	-0.044121	4.320862
213.284278	6403.678476	8.250048	-0.044147	4.323455
213.307294	6411.745472	8.255053	-0.044157	4.326084
213.532729	6419.712233	8.260058	-0.044205	4.328680
213.622389	6427.802948	8.265062	-0.044227	4.331314
213.947953	6435.814783	8.270067	-0.044293	4.333923
214.186030	6443.799845	8.275072	-0.044343	4.336520
214.156283	6451.836842	8.280077	-0.044343	4.339131
214.160075	6459.842381	8.285082	-0.044349	4.341730
214.403451	6467.817875	8.290086	-0.044399	4.344320
214.498341	6475.888945	8.295091	-0.044423	4.346938
214.669821	6483.881451	8.300096	-0.044460	4.349530
214.777230	6491.968805	8.305101	-0.044485	4.352150
214.817587	6500.006483	8.310106	-0.044498	4.354752
215.135077	6508.004848	8.315110	-0.044563	4.357342
215.192939	6515.951423	8.320115	-0.044579	4.359912
215.221866	6523.931310	8.325120	-0.044590	4.362491
215.142646	6531.941244	8.330125	-0.044581	4.365077
215.418660	6539.978116	8.335130	-0.044637	4.367672
215.728818	6547.967925	8.340134	-0.044701	4.370252
215.864391	6556.054994	8.345139	-0.044731	4.372859
215.989511	6564.044398	8.350144	-0.044760	4.375434
216.338540	6572.141134	8.355149	-0.044831	4.378043
216.580065	6580.046825	8.360154	-0.044881	4.380588
216.717010	6588.048441	8.365158	-0.044912	4.383163
216.939857	6596.088271	8.370163	-0.044959	4.385748
217.131155	6604.092665	8.375168	-0.045000	4.388320
217.137556	6612.153703	8.380173	-0.045006	4.390908
217.324621	6620.147283	8.385178	-0.045047	4.393474
217.641237	6628.215483	8.390182	-0.045111	4.396062
217.822609	6636.196323	8.395187	-0.045150	4.398621
217.756960	6644.206482	8.400192	-0.045144	4.401186
218.037215	6652.184379	8.405197	-0.045201	4.403741
217.973040	6660.237064	8.410202	-0.045195	4.406317
218.132821	6668.248841	8.415206	-0.045230	4.408879
218.290271	6676.305460	8.420211	-0.045265	4.411454
218.525776	6684.284462	8.425216	-0.045314	4.414003
218.703822	6692.324845	8.430221	-0.045353	4.416570
218.706670	6700.308043	8.435226	-0.045358	4.419116
219.040487	6708.372170	8.440230	-0.045426	4.421688
219.040736	6716.379449	8.445235	-0.045432	4.424239
219.135673	6724.399773	8.450240	-0.045455	4.426793
219.503423	6732.424740	8.455245	-0.045529	4.429349
219.522054	6740.486990	8.460250	-0.045538	4.431913
219.651174	6748.523871	8.465254	-0.045567	4.434468
219.852324	6756.520204	8.470259	-0.045610	4.437009
219.846409	6764.462081	8.475264	-0.045614	4.439530
219.928497	6772.500789	8.480269	-0.045635	4.442081
220.066467	6780.456750	8.485274	-0.045666	4.444605
220.207855	6788.536479	8.490278	-0.045698	4.447166
220.401533	6796.534476	8.495283	-0.045739	4.449700
220.334559	6804.608514	8.500288	-0.045732	4.452256
220.573884	6812.611266	8.505293	-0.045782	4.454789
220.700748	6820.633894	8.510298	-0.045811	4.457326
220.769209	6828.598619	8.515302	-0.045830	4.459843
221.180261	6836.654738	8.520307	-0.045912	4.462389
221.216235	6844.597375	8.525312	-0.045924	4.464897
221.243090	6852.675269	8.530317	-0.045934	4.467445
221.334027	6860.685752	8.535322	-0.045957	4.469971
221.748485	6868.718986	8.540326	-0.046039	4.472504
221.842076	6876.734699	8.545331	-0.046062	4.475029
221.814893	6884.712635	8.550336	-0.046062	4.477540
221.950525	6892.752880	8.555341	-0.046093	4.480070
222.177222	6900.748111	8.560346	-0.046141	4.482584
222.092201	6908.716335	8.565351	-0.046130	4.485088
222.233215	6916.798088	8.570355	-0.046162	4.487626
222.442971	6924.768389	8.575360	-0.046207	4.490128
222.711066	6932.852171	8.580365	-0.046262	4.492665
222.837329	6940.829419	8.585370	-0.046291	4.495166
222.802063	6948.841567	8.590375	-0.046290	4.497677
223.124202	6956.888850	8.595379	-0.046355	4.500198
223.116073	6964.871871	8.600384	-0.046359	4.502696
223.254713	6972.876028	8.605389	-0.046390	4.505200
223.493372	6980.896837	8.610394	-0.046440	4.507709
223.524523	6988.944925	8.615399	-0.046452	4.510223
223.678307	6997.038533	8.620403	-0.046486	4.512751
223.976837	7005.019539	8.625408	-0.046547	4.515243
224.054651	7013.006778	8.630413	-0.046567	4.517735
224.050648	7020.979046	8.635418	-0.046571	4.520220
224.180679	7028.957734	8.640423	-0.046601	4.522706
224.474712	7037.025945	8.645427	-0.046661	4.525220
224.501301	7045.030383	8.650432	-0.046671	4.527711
224.777251	7053.055639	8.655437	-0.046728	4.530208
224.856364	7061.090745	8.660442	-0.046749	4.532706
224.887936	7069.093438	8.665447	-0.046760	4.535193
225.187411	7077.103924	8.670451	-0.046821	4.537681
225.267205	7085.087039	8.675456	-0.046841	4.540159
225.489270	7093.095881	8.680461	-0.046888	4.542644
225.560496	7101.109036	8.685466	-0.046907	4.545128
225.562222	7109.158227	8.690471	-0.046913	4.547623
225.807829	7117.192433	8.695475	-0.046964	4.550111
225.782158	7125.210297	8.700480	-0.046964	4.552593
225.908336	7133.279253	8.705485	-0.046993	4.555089
226.146775	7141.243094	8.710490	-0.047043	4.557552
226.363703	7149.185163	8.715495	-0.047089	4.560006
226.323659	7157.282332	8.720499	-0.047087	4.562507
226.496248	7165.220201	8.725504	-0.047125	4.564957
226.697409	7173.280733	8.730509	-0.047167	4.567444
226.775249	7181.275297	8.735514	-0.047187	4.569910
226.949051	7189.368128	8.740519	-0.047225	4.572404
226.966836	7197.387888	8.745523	-0.047234	4.574874
227.079773	7205.392435	8.750528	-0.047260	4.577338
227.399768	7213.393654	8.755533	-0.047325	4.579800
227.623368	7221.428002	8.760538	-0.047373	4.582271
227.635837	7229.387027	8.765543	-0.047380	4.584717
227.815481	7237.442453	8.770547	-0.047419	4.587191
227.834024	7245.425333	8.775552	-0.047428	4.589642
227.888708	7253.516237	8.780557	-0.047444	4.592125
228.057826	7261.540078	8.785562	-0.047481	4.594586
228.154234	7269.559231	8.790567	-0.047504	4.597043
228.578150	7277.480362	8.795571	-0.047588	4.599470
228.406262	7285.566630	8.800576	-0.047562	4.601946
228.621898	7293.510915	8.805581	-0.047607	4.604377
228.747453	7301.548384	8.810586	-0.047636	4.606835
228.987683	7309.531915	8.815591	-0.047686	4.609276
229.224325	7317.619950	8.820595	-0.047736	4.611747
229.314484	7325.613240	8.825600	-0.047758	4.614188
229.540656	7333.653791	8.830605	-0.047806	4.616642
229.642107	7341.639303	8.835610	-0.047830	4.619077
229.681405	7349.657730	8.840615	-0.047843	4.621522
230.039512	7357.675513	8.845619	-0.047915	4.623965
230.121305	7365.686167	8.850624	-0.047936	4.626404
230.226770	7373.700088	8.855629	-0.047961	4.628844
230.495005	7381.728753	8.860634	-0.048016	4.631286
230.691983	7389.771938	8.865639	-0.048058	4.633731
230.922627	7397.829787	8.870643	-0.048107	4.636180
231.122897	7405.718180	8.875648	-0.048149	4.638576
231.046246	7413.750077	8.880653	-0.048140	4.641014
230.981706	7421.720332	8.885658	-0.048134	4.643432
231.226997	7429.792273	8.890663	-0.048185	4.645880
231.392774	7437.819942	8.895667	-0.048221	4.648313
231.359701	7445.819374	8.900672	-0.048221	4.650736
231.752245	7453.886135	8.905677	-0.048299	4.653178
231.807137	7461.925258	8.910682	-0.048315	4.655611
232.022820	7469.893787	8.915687	-0.048360	4.658021
232.158061	7477.940625	8.920691	-0.048391	4.660453
232.105751	7485.859753	8.925696	-0.048387	4.662846
232.490520	7493.909802	8.930701	-0.048464	4.665276
232.414779	7501.936420	8.935706	-0.048455	4.667699
232.420550	7509.923029	8.940711	-0.048462	4.670108
232.818051	7518.048134	8.945715	-0.048541	4.672558
232.815007	7526.098038	8.950720	-0.048546	4.674983
232.937361	7534.046994	8.955725	-0.048574	4.677377
232.988149	7542.016308	8.960730	-0.048589	4.679776
233.145934	7550.037015	8.965735	-0.048624	4.682189
233.406601	7558.019922	8.970739	-0.048678	4.684589
233.245476	7566.039942	8.975744	-0.048653	4.687000
233.482679	7574.072633	8.980749	-0.048703	4.689413
233.581695	7582.102475	8.985754	-0.048727	4.691824
233.841517	7590.057382	8.990759	-0.048781	4.694211
233.926574	7598.168356	8.995763	-0.048802	4.696643
233.982109	7606.068795	9.000768	-0.048818	4.699012
234.141824	7614.159477	9.005773	-0.048853	4.701435
234.332561	7622.091958	9.010778	-0.048894	4.703811
234.592649	7630.173006	9.015783	-0.048948	4.706229
234.746392	7638.248131	9.020787	-0.048982	4.708644
234.681737	7646.183762	9.025792	-0.048975	4.711018
234.998983	7654.304013	9.030797	-0.049040	4.713444
235.055486	7662.249798	9.035802	-0.049056	4.715817
235.106840	7670.199573	9.040807	-0.049071	4.718190
235.488468	7678.323609	9.045811	-0.049147	4.720614
235.498143	7686.280187	9.050816	-0.049154	4.722987
235.588894	7694.321109	9.055821	-0.049177	4.725383
235.501332	7702.371883	9.060826	-0.049166	4.727782
235.722407	7710.334144	9.065831	-0.049213	4.730153
235.897194	7718.385038	9.070835	-0.049251	4.732549
236.152498	7726.403073	9.075840	-0.049304	4.734933
236.288880	7734.393632	9.080845	-0.049334	4.737309
236.307432	7742.418607	9.085850	-0.049343	4.739694
236.351744	7750.374311	9.090855	-0.049357	4.742057
236.621552	7758.455208	9.095859	-0.049413	4.744455
236.775240	7766.493826	9.100864	-0.049447	4.746840
236.907927	7774.492106	9.105869	-0.049477	4.749212
237.112285	7782.522619	9.110874	-0.049520	4.751592
237.192335	7790.522129	9.115879	-0.049541	4.753962
237.338036	7798.589686	9.120883	-0.049573	4.756350
237.328478	7806.517139	9.125888	-0.049577	4.758697
237.751629	7814.544375	9.130893	-0.049661	4.761070
237.440710	7822.532161	9.135898	-0.049609	4.763433
237.630452	7830.524601	9.140903	-0.049649	4.765795
238.152407	7838.608701	9.145907	-0.049752	4.768181
238.115727	7846.598038	9.150912	-0.049751	4.770540
238.055438	7854.611128	9.155917	-0.049745	4.772905
238.233669	7862.681022	9.160922	-0.049784	4.775284
238.448804	7870.626273	9.165927	-0.049829	4.777626
238.541896	7878.709538	9.170931	-0.049852	4.780007
238.644816	7886.649628	9.175936	-0.049876	4.782345
239.031579	7894.624062	9.180941	-0.049954	4.784691
239.142012	7902.708045	9.185946	-0.049980	4.787069
238.913180	7910.693623	9.190951	-0.049943	4.789419
239.397592	7918.763354	9.195955	-0.050038	4.791788
239.364533	7926.773442	9.200960	-0.050038	4.794142
239.649253	7934.822967	9.205965	-0.050096	4.796504
239.622343	7942.715534	9.210970	-0.050096	4.798821
239.819754	7950.777100	9.215975	-0.050139	4.801185
239.980201	7958.778256	9.220979	-0.050174	4.803530
240.004864	7966.846292	9.225984	-0.050184	4.805894
240.066416	7974.831477	9.230989	-0.050201	4.808233
240.062942	7982.892081	9.235994	-0.050206	4.810593
240.209292	7990.347586	9.240999	-0.050238	4.812774
240.321373	7995.003760	9.246003	-0.050262	4.814135

240.513189	7997.381000	9.251008	-0.050300	4.814830
240.344356	7998.680777	9.256013	-0.050269	4.815211
240.571834	7999.379554	9.261018	-0.050312	4.815414
240.879183	7999.698479	9.266023	-0.050370	4.815506
240.830677	7999.726539	9.271027	-0.050361	4.815514
240.603145	7999.735671	9.276032	-0.050319	4.815518
240.864349	7999.743140	9.281037	-0.050368	4.815519
241.035182	7999.776902	9.286042	-0.050400	4.815528
240.903721	7999.695770	9.291047	-0.050376	4.815505
240.899937	7999.760860	9.296051	-0.050375	4.815524
240.904911	7999.988391	9.301056	-0.050377	4.815590
241.160123	7999.971206	9.306061	-0.050424	4.815584
241.071862	8000.040262	9.311066	-0.050408	4.815605
240.906211	8000.086704	9.316071	-0.050378	4.815619
241.172069	7999.931951	9.321075	-0.050427	4.815572
241.091619	8000.044912	9.326080	-0.050412	4.815606
241.104600	7999.998160	9.331085	-0.050415	4.815592
241.246022	8000.208696	9.336090	-0.050442	4.815653
241.225916	8000.011918	9.341095	-0.050438	4.815596
241.384797	7999.829798	9.346099	-0.050468	4.815542
241.333838	8000.169607	9.351104	-0.050459	4.815641
241.387651	7999.886474	9.356109	-0.050469	4.815558
241.370784	8000.111518	9.361114	-0.050466	4.815624
241.550576	8000.167852	9.366119	-0.050500	4.815640
241.793512	7999.930506	9.371123	-0.050545	4.815569
241.466258	8000.077892	9.376128	-0.050484	4.815614
241.575762	7999.841580	9.381133	-0.050505	4.815544
241.683124	7999.977885	9.386138	-0.050525	4.815583
241.688168	7999.960901	9.391143	-0.050526	4.815578
241.774705	7999.856619	9.396147	-0.050543	4.815547
241.633407	7999.944032	9.401152	-0.050517	4.815574
241.682978	7999.937383	9.406157	-0.050526	4.815572
241.809892	7999.876468	9.411162	-0.050550	4.815553
241.928866	7999.876288	9.416167	-0.050572	4.815552
242.056960	7999.800443	9.421171	-0.050596	4.815530
241.917709	7999.946618	9.426176	-0.050571	4.815573
241.955599	7999.856492	9.431181	-0.050578	4.815547
242.026569	7999.858734	9.436186	-0.050591	4.815547
241.821121	7999.898121	9.441191	-0.050553	4.815559
241.805241	7999.871187	9.446195	-0.050550	4.815552
242.086082	7999.964402	9.451200	-0.050603	4.815577
242.052803	7999.863508	9.456205	-0.050597	4.815548
241.953067	7999.872582	9.461210	-0.050579	4.815551
241.930900	7999.957663	9.466215	-0.050575	4.815576
242.003584	7999.889459	9.471219	-0.050588	4.815556
242.005772	7999.872429	9.476224	-0.050589	4.815551
241.955013	7999.937824	9.481229	-0.050580	4.815570
242.124828	7999.895760	9.486234	-0.050612	4.815557
242.178389	8000.058955	9.491239	-0.050622	4.815605
242.253942	7999.889357	9.496243	-0.050636	4.815555
242.356487	7999.852604	9.501248	-0.050655	4.815543
242.205204	7999.963347	9.506253	-0.050628	4.815577
242.233428	8000.022554	9.511258	-0.050633	4.815594
242.217850	7999.849338	9.516263	-0.050630	4.815543
242.563977	7999.778108	9.521267	-0.050695	4.815521
242.455394	7999.889546	9.526272	-0.050675	4.815554
242.234958	7999.840063	9.531277	-0.050634	4.815540
242.299383	7999.900927	9.536282	-0.050646	4.815558
242.192098	7999.948318	9.541287	-0.050627	4.815572
242.303909	7999.854056	9.546291	-0.050648	4.815544
242.384875	7999.882087	9.551296	-0.050663	4.815552
242.437702	7999.873356	9.556301	-0.050673	4.815549
242.317757	7999.870355	9.561306	-0.050651	4.815549
242.099491	7999.896721	9.566311	-0.050611	4.815557
242.283620	7999.829262	9.571315	-0.050645	4.815537
242.292579	7999.981053	9.576320	-0.050647	4.815581
242.055485	7999.870435	9.581325	-0.050603	4.815550
242.181004	7999.878903	9.586330	-0.050627	4.815552
242.380653	7999.853341	9.591335	-0.050664	4.815543
242.452274	7999.879085	9.596339	-0.050677	4.815551
242.330616	7999.976428	9.601344	-0.050655	4.815580
242.468159	7999.932771	9.606349	-0.050681	4.815566
242.252345	7999.887634	9.611354	-0.050641	4.815554
242.317517	7999.832121	9.616359	-0.050653	4.815537
242.406571	7999.877368	9.621363	-0.050670	4.815550
242.299156	7999.939707	9.626368	-0.050650	4.815569
242.242203	7999.896088	9.631373	-0.050640	4.815557
242.556201	7999.909759	9.636378	-0.050699	4.815559
242.331117	7999.878352	9.641383	-0.050657	4.815551
242.344940	7999.838020	9.646387	-0.050660	4.815539
242.286644	8000.013276	9.651392	-0.050649	4.815591
242.740600	7999.860515	9.656397	-0.050734	4.815544
242.814006	7999.825423	9.661402	-0.050748	4.815533
242.594487	7999.917971	9.666407	-0.050707	4.815561
242.824143	7999.844847	9.671411	-0.050750	4.815539
242.623627	7999.859755	9.676416	-0.050713	4.815544
242.642514	7999.862217	9.681421	-0.050717	4.815545
242.734636	7999.861600	9.686426	-0.050734	4.815544
242.746660	7999.931222	9.691431	-0.050736	4.815564
242.832771	7999.776744	9.696435	-0.050753	4.815519
242.556020	7999.896123	9.701440	-0.050701	4.815555
242.663246	7999.794311	9.706445	-0.050722	4.815525
242.612424	7999.930181	9.711450	-0.050712	4.815565
242.679306	7999.760441	9.716455	-0.050725	4.815515
242.884988	7999.874859	9.721459	-0.050764	4.815547
242.711534	7999.793037	9.726464	-0.050731	4.815524
242.707458	7999.881617	9.731469	-0.050731	4.815550
242.819706	7999.826870	9.736474	-0.050752	4.815533
243.072101	7999.873709	9.741479	-0.050799	4.815546
242.917812	7999.832776	9.746483	-0.050771	4.815535
242.806676	7999.887580	9.751488	-0.050750	4.815551
242.865726	7999.762560	9.756493	-0.050761	4.815514
242.903053	7999.908407	9.761498	-0.050769	4.815557
242.889893	7999.852686	9.766503	-0.050766	4.815541
242.948573	7999.818423	9.771507	-0.050778	4.815530
243.040250	7999.802849	9.776512	-0.050795	4.815525
243.137058	7999.848224	9.781517	-0.050813	4.815538
243.076029	7999.808809	9.786522	-0.050802	4.815527
242.987663	7999.892814	9.791527	-0.050786	4.815552
242.971741	7999.787929	9.796531	-0.050783	4.815521
242.819081	7999.962719	9.801536	-0.050755	4.815573
242.792729	7999.791461	9.806541	-0.050750	4.815523
242.917069	7999.844758	9.811546	-0.050773	4.815538
242.864914	7999.859945	9.816551	-0.050764	4.815543
242.886803	7999.865659	9.821555	-0.050768	4.815544
243.145106	7999.885900	9.826560	-0.050817	4.815549
243.314262	7999.755197	9.831565	-0.050848	4.815510
243.031672	7999.836041	9.836570	-0.050796	4.815535
243.078900	7999.877405	9.841575	-0.050805	4.815547
243.273658	7999.887002	9.846579	-0.050841	4.815549
243.019413	7999.811339	9.851584	-0.050794	4.815528
243.058527	7999.842961	9.856589	-0.050802	4.815537
243.169051	7999.936611	9.861594	-0.050823	4.815564
243.005799	7999.851751	9.866599	-0.050792	4.815540
243.128515	7999.822801	9.871603	-0.050815	4.815531
243.043450	7999.996557	9.876608	-0.050800	4.815582
243.255373	7999.847329	9.881613	-0.050839	4.815537
243.038638	7999.833141	9.886618	-0.050799	4.815534
242.849047	7999.855702	9.891623	-0.050764	4.815542
243.009026	7999.786782	9.896627	-0.050794	4.815521
242.781536	7999.911235	9.901632	-0.050752	4.815558
242.861615	7999.826065	9.906637	-0.050767	4.815533
243.116610	7999.796065	9.911642	-0.050815	4.815523
242.899730	7999.943115	9.916647	-0.050775	4.815567
243.058754	7999.750314	9.921651	-0.050805	4.815510
243.103778	7999.889881	9.926656	-0.050813	4.815550
243.015169	7999.953594	9.931661	-0.050797	4.815569
243.047707	7999.760869	9.936666	-0.050803	4.815513
243.106306	7999.936963	9.941671	-0.050814	4.815564
243.286617	7999.844882	9.946675	-0.050848	4.815536
243.001318	7999.973733	9.951680	-0.050795	4.815575
243.034736	7999.829074	9.956685	-0.050802	4.815533
243.170593	7999.967985	9.961690	-0.050827	4.815573
243.009811	8000.105270	9.966695	-0.050798	4.815614
243.016822	7999.840585	9.971699	-0.050799	4.815536
243.123798	7999.855160	9.976704	-0.050819	4.815540
243.157628	7999.832238	9.981709	-0.050826	4.815533
243.075429	7999.868292	9.986714	-0.050811	4.815544
243.065028	7999.847853	9.991719	-0.050809	4.815538
243.079727	7999.834230	9.996723	-0.050812	4.815534
243.034593	7999.864481	10.001728	-0.050804	4.815543
243.206470	7999.876908	10.006733	-0.050836	4.815546
243.488546	8000.036354	10.011738	-0.050889	4.815591
243.420216	8000.099331	10.016743	-0.050876	4.815610
243.266401	7999.795720	10.021747	-0.050848	4.815522
243.413290	7999.978591	10.026752	-0.050875	4.815575
243.387241	7999.765691	10.031757	-0.050871	4.815513
243.321505	7999.836183	10.036762	-0.050859	4.815533
243.106781	7999.973658	10.041767	-0.050819	4.815575
243.221428	7999.899729	10.046771	-0.050840	4.815552
243.338381	7999.885635	10.051776	-0.050862	4.815548
243.165885	7999.941575	10.056781	-0.050830	4.815565
243.525424	7999.870565	10.061786	-0.050898	4.815542
243.625368	7999.948027	10.066791	-0.050916	4.815565
243.482624	7999.819719	10.071795	-0.050890	4.815528
243.612736	7999.930774	10.076800	-0.050915	4.815560
243.362596	7999.961959	10.081805	-0.050868	4.815570
243.557832	7999.782559	10.086810	-0.050905	4.815517
243.383592	7999.850218	10.091815	-0.050872	4.815537
243.534522	7999.769404	10.096819	-0.050901	4.815513
243.497259	7999.886277	10.101824	-0.050894	4.815547
243.233317	7999.863846	10.106829	-0.050845	4.815542
243.406301	7999.769510	10.111834	-0.050878	4.815513
243.409819	7999.963929	10.116839	-0.050879	4.815570
243.369863	7999.831956	10.121843	-0.050871	4.815532
243.395734	7999.905008	10.126848	-0.050876	4.815553
243.406316	7999.825113	10.131853	-0.050878	4.815530
243.255301	7999.784232	10.136858	-0.050851	4.815518
243.209512	7999.844371	10.141863	-0.050842	4.815536
243.473358	7999.808108	10.146867	-0.050892	4.815524
243.487590	8000.002703	10.151872	-0.050895	4.815581
243.455490	7999.834551	10.156877	-0.050889	4.815532
243.634432	7999.849230	10.161882	-0.050922	4.815536
243.630056	7999.821414	10.166887	-0.050922	4.815528
243.532045	7999.839058	10.171891	-0.050904	4.815533
243.359954	7999.936651	10.176896	-0.050872	4.815562
243.473366	7999.848819	10.181901	-0.050893	4.815536
243.556619	7999.807481	10.186906	-0.050909	4.815524
243.375972	7999.856882	10.191911	-0.050875	4.815539
243.362768	7999.769126	10.196915	-0.050873	4.815513
243.443079	7999.864420	10.201920	-0.050888	4.815541
243.359806	7999.818235	10.206925	-0.050873	4.815528
243.446996	7999.901895	10.211930	-0.050890	4.815552
243.400301	7999.876594	10.216935	-0.050881	4.815545
243.465574	7999.754877	10.221939	-0.050893	4.815509
243.465895	7999.867022	10.226944	-0.050894	4.815542
243.475662	7999.855454	10.231949	-0.050896	4.815538
243.656494	7999.771924	10.236954	-0.050930	4.815513
243.383960	7999.951171	10.241959	-0.050879	4.815567
243.438085	7999.818594	10.246963	-0.050889	4.815528
243.422658	7999.797006	10.251968	-0.050887	4.815521
243.382865	7999.962957	10.256973	-0.050880	4.815570
243.504791	7999.860315	10.261978	-0.050902	4.815539
243.455192	7999.856323	10.266983	-0.050893	4.815538
243.673553	7999.821455	10.271987	-0.050934	4.815527
243.560281	7999.917870	10.276992	-0.050914	4.815556
243.571366	8000.106008	10.281997	-0.050916	4.815611
243.536346	7999.858788	10.287002	-0.050909	4.815539
243.469824	7999.854521	10.292007	-0.050897	4.815538
243.685347	7999.784369	10.297011	-0.050938	4.815516
243.684437	7999.866596	10.302016	-0.050938	4.815540
243.382529	7999.875581	10.307021	-0.050882	4.815544
243.596231	7999.839570	10.312026	-0.050922	4.815533
243.511655	7999.895874	10.317031	-0.050906	4.815550
243.744791	7999.808925	10.322035	-0.050950	4.815523
243.563968	7999.833763	10.327040	-0.050916	4.815531
243.717114	7999.801037	10.332045	-0.050945	4.815521
243.747693	7999.913676	10.337050	-0.050951	4.815554
243.563538	7999.790033	10.342055	-0.050917	4.815518
243.611905	7999.865587	10.347059	-0.050926	4.815540
243.607682	7999.816417	10.352064	-0.050926	4.815526
243.560774	7999.866928	10.357069	-0.050917	4.815541
243.717501	7999.739225	10.362074	-0.050946	4.815503
243.559623	7999.900050	10.367079	-0.050917	4.815551
243.596369	7999.845140	10.372083	-0.050924	4.815534
243.490106	7999.877600	10.377088	-0.050905	4.815544
243.749289	7999.751564	10.382093	-0.050953	4.815506
243.936057	7999.843254	10.387098	-0.050988	4.815532
243.676337	7999.976794	10.392103	-0.050940	4.815572
243.647395	7999.826846	10.397107	-0.050935	4.815529
243.691985	7999.866033	10.402112	-0.050943	4.815540
243.700599	7999.839496	10.407117	-0.050945	4.815532
243.720305	7999.742665	10.412122	-0.050949	4.815504
243.710717	7999.946482	10.417127	-0.050948	4.815563
243.873271	7999.823144	10.422131	-0.050978	4.815527
243.819488	7999.899171	10.427136	-0.050968	4.815549
243.547717	7999.830696	10.432141	-0.050918	4.815530
243.897698	7999.803311	10.437146	-0.050983	4.815521
243.804901	7999.955586	10.442151	-0.050966	4.815566
243.831160	7999.745671	10.447155	-0.050971	4.815504
243.905517	7999.850480	10.452160	-0.050985	4.815534
243.882692	7999.944097	10.457165	-0.050981	4.815562
243.965731	7999.851499	10.462170	-0.050997	4.815534
243.947885	7999.764733	10.467175	-0.050994	4.815509
243.803305	7999.921504	10.472179	-0.050967	4.815556
243.649996	7999.929705	10.477184	-0.050939	4.815559
243.733731	7999.735676	10.482189	-0.050955	4.815502
243.872181	7999.837257	10.487194	-0.050981	4.815531
243.674970	7999.918423	10.492199	-0.050944	4.815555
243.708235	7999.742792	10.497203	-0.050951	4.815504
243.854753	7999.814606	10.502208	-0.050978	4.815524
243.996448	7999.969633	10.507213	-0.051005	4.815569
243.749971	7999.792649	10.512218	-0.050959	4.815518
243.799764	7999.984621	10.517223	-0.050969	4.815574
244.147536	7999.802365	10.522227	-0.051033	4.815519
243.919866	7999.858475	10.527232	-0.050991	4.815537
243.950729	7999.927338	10.532237	-0.050997	4.815557
243.981022	7999.792235	10.537242	-0.051003	4.815517
243.859529	7999.954722	10.542247	-0.050981	4.815565
243.732465	7999.799972	10.547251	-0.050957	4.815520
244.105903	7999.784716	10.552256	-0.051027	4.815514
243.979510	7999.827526	10.557261	-0.051004	4.815527
244.069196	7999.826870	10.562266	-0.051021	4.815527
243.851335	7999.939735	10.567271	-0.050980	4.815561
243.988377	7999.740165	10.572275	-0.051006	4.815502
244.115880	7999.967574	10.577280	-0.051030	4.815567
243.898819	7999.822036	10.582285	-0.050990	4.815526
243.927683	7999.795829	10.587290	-0.050995	4.815518
243.816234	7999.940326	10.592295	-0.050975	4.815561
243.745370	7999.739508	10.597299	-0.050962	4.815503
244.044766	7999.875745	10.602304	-0.051018	4.815541
243.638149	7999.905448	10.607309	-0.050942	4.815552
243.845009	7999.818071	10.612314	-0.050981	4.815525
243.778775	7999.873606	10.617319	-0.050969	4.815542
244.164709	7999.776330	10.622323	-0.051041	4.815511
244.180142	7999.874842	10.627328	-0.051044	4.815540
243.913978	7999.806456	10.632333	-0.050995	4.815521
243.916619	7999.794772	10.637338	-0.050996	4.815518
244.144392	7999.922370	10.642343	-0.051038	4.815554
244.109392	7999.781932	10.647347	-0.051032	4.815513
244.121004	7999.834464	10.652352	-0.051034	4.815528
244.162143	7999.863985	10.657357	-0.051042	4.815537
243.931101	7999.783357	10.662362	-0.050999	4.815514
243.850593	7999.860017	10.667367	-0.050985	4.815537
243.947356	7999.768710	10.672371	-0.051003	4.815510
243.936847	7999.958633	10.677376	-0.051001	4.815566
244.066912	7999.783509	10.682381	-0.051025	4.815514
244.044700	7999.806659	10.687386	-0.051022	4.815521
243.905381	7999.889836	10.692391	-0.050996	4.815546
243.737529	7999.779271	10.697395	-0.050965	4.815514
244.002154	7999.842330	10.702400	-0.051014	4.815531
244.040760	7999.877148	10.707405	-0.051022	4.815541
244.090405	7999.834195	10.712410	-0.051031	4.815528
243.934814	7999.798577	10.717415	-0.051002	4.815519
244.104976	7999.859031	10.722419	-0.051034	4.815536
244.267968	7999.849958	10.727424	-0.051065	4.815532
244.159700	7999.819382	10.732429	-0.051045	4.815524
244.224719	7999.755322	10.737434	-0.051057	4.815505
244.072515	7999.889546	10.742439	-0.051029	4.815545
244.020763	7999.744564	10.747443	-0.051020	4.815503
244.219155	7999.890904	10.752448	-0.051057	4.815544
244.234023	7999.829231	10.757453	-0.051060	4.815526
244.014320	7999.832079	10.762458	-0.051019	4.815528
243.969238	7999.884755	10.767463	-0.051011	4.815544
244.050743	7999.751555	10.772467	-0.051026	4.815504
244.091954	7999.910285	10.777472	-0.051034	4.815551
243.991981	7999.807231	10.782477	-0.051016	4.815521
243.993875	7999.911929	10.787482	-0.051017	4.815552
244.121033	7999.863831	10.792487	-0.051040	4.815537
244.189506	7999.763520	10.797491	-0.051053	4.815507
244.030872	7999.818619	10.802496	-0.051024	4.815524
244.109582	7999.855159	10.807501	-0.051039	4.815534
244.301884	7999.817732	10.812506	-0.051075	4.815523
244.063556	7999.805327	10.817511	-0.051031	4.815520
244.205145	7999.810855	10.822515	-0.051057	4.815521
244.195904	7999.885473	10.827520	-0.051056	4.815543
243.983874	7999.926888	10.832525	-0.051017	4.815556
244.027067	7999.841115	10.837530	-0.051025	4.815531
244.124148	7999.748746	10.842535	-0.051043	4.815503
244.029487	7999.879635	10.847539	-0.051026	4.815542
243.963844	7999.878585	10.852544	-0.051014	4.815542
243.904877	7999.774064	10.857549	-0.051003	4.815512
244.097206	7999.818861	10.862554	-0.051039	4.815524
243.961603	7999.880742	10.867559	-0.051014	4.815542
244.066576	7999.816264	10.872563	-0.051034	4.815523
244.112847	7999.831987	10.877568	-0.051043	4.815528
243.880522	7999.998008	10.882573	-0.051000	4.815577
244.028929	7999.777267	10.887578	-0.051027	4.815512
244.111732	7999.879011	10.892583	-0.051043	4.815541
244.083603	7999.773924	10.897587	-0.051038	4.815511
244.152133	7999.859418	10.902592	-0.051051	4.815535
244.057251	7999.844010	10.907597	-0.051034	4.815531
244.043077	7999.771185	10.912602	-0.051031	4.815510
243.992132	7999.904922	10.917607	-0.051022	4.815549
244.023290	7999.844582	10.922611	-0.051028	4.815532
244.188647	7999.825937	10.927616	-0.051059	4.815525
244.038718	7999.864092	10.932621	-0.051031	4.815537
244.039121	7999.765877	10.937626	-0.051031	4.815508
244.240129	7999.890904	10.942631	-0.051069	4.815544
244.148150	7999.764488	10.947635	-0.051052	4.815508
243.962193	7999.826616	10.952640	-0.051018	4.815527
244.031513	7999.873681	10.957645	-0.051031	4.815540
244.088011	7999.848992	10.962650	-0.051042	4.815532
244.055735	7999.835672	10.967655	-0.051036	4.815529
244.218390	7999.840476	10.972659	-0.051066	4.815529
244.263893	7999.828422	10.977664	-0.051075	4.815526
244.217804	7999.764688	10.982669	-0.051067	4.815507
244.318796	7999.887018	10.987674	-0.051086	4.815542
244.301834	7999.802401	10.992679	-0.051083	4.815518
244.529814	7999.878747	10.997683	-0.051125	4.815539
244.477950	7999.825597	11.002688	-0.051116	4.815524
244.114985	7999.846400	11.007693	-0.051049	4.815532
244.380039	7999.786666	11.012698	-0.051098	4.815513
244.064180	7999.889392	11.017703	-0.051040	4.815544
244.100985	7999.847297	11.022707	-0.051047	4.815532
244.273008	7999.877882	11.027712	-0.051079	4.815540
244.121375	7999.736612	11.032717	-0.051051	4.815499
243.979407	7999.865663	11.037722	-0.051025	4.815538
244.316473	7999.905343	11.042727	-0.051088	4.815548
244.401424	7999.738027	11.047731	-0.051104	4.815498
244.392244	7999.900209	11.052736	-0.051102	4.815546
244.290049	7999.863324	11.057741	-0.051083	4.815536
244.192374	7999.784868	11.062746	-0.051065	4.815513
244.184803	7999.816799	11.067751	-0.051064	4.815523
244.199962	7999.873660	11.072755	-0.051067	4.815539
244.249945	7999.824305	11.077760	-0.051077	4.815524
244.099476	7999.777024	11.082765	-0.051049	4.815511
244.297752	7999.806969	11.087770	-0.051086	4.815519
244.385653	7999.859676	11.092775	-0.051103	4.815534
244.427335	7999.876392	11.097779	-0.051111	4.815539
244.238436	7999.791110	11.102784	-0.051076	4.815515
244.020343	7999.858054	11.107789	-0.051035	4.815535
244.276591	7999.791770	11.112794	-0.051083	4.815515
244.144664	7999.903899	11.117799	-0.051059	4.815548
244.163063	7999.805976	11.122803	-0.051063	4.815519
244.230209	7999.793207	11.127808	-0.051075	4.815515
244.234714	7999.900084	11.132813	-0.051076	4.815547
244.386269	7999.820348	11.137818	-0.051105	4.815523
244.472523	7999.782261	11.142823	-0.051121	4.815511
244.420472	7999.797450	11.147827	-0.051112	4.815516
244.290401	7999.963003	11.152832	-0.051088	4.815565
244.214036	7999.851790	11.157837	-0.051074	4.815532
244.415234	7999.847611	11.162842	-0.051111	4.815530
244.242162	7999.896068	11.167847	-0.051079	4.815545
244.052036	7999.869497	11.172851	-0.051044	4.815538
244.084058	7999.824121	11.177856	-0.051050	4.815525
244.136144	7999.780139	11.182861	-0.051060	4.815512
244.230613	7999.909838	11.187866	-0.051078	4.815549
244.234721	7999.830903	11.192871	-0.051079	4.815526
244.274618	7999.848658	11.197875	-0.051087	4.815531
244.026709	7999.819011	11.202880	-0.051041	4.815524
243.964505	7999.793457	11.207885	-0.051029	4.815517
244.228766	7999.803119	11.212890	-0.051079	4.815518
244.014165	7999.853035	11.217895	-0.051039	4.815534
244.056861	7999.886852	11.222899	-0.051047	4.815543
244.271936	7999.840186	11.227904	-0.051087	4.815529
244.084283	7999.802978	11.232909	-0.051053	4.815519
244.013046	7999.791158	11.237914	-0.051040	4.815516
243.989371	7999.873015	11.242919	-0.051036	4.815540
244.288006	7999.837320	11.247923	-0.051091	4.815528
244.241498	7999.796004	11.252928	-0.051083	4.815516
244.144895	7999.927930	11.257933	-0.051065	4.815555
244.163759	7999.772352	11.262938	-0.051069	4.815509
244.187328	7999.844300	11.267943	-0.051073	4.815530
244.131797	7999.843414	11.272947	-0.051063	4.815530
244.446214	7999.774873	11.277952	-0.051122	4.815509
244.340142	7999.857525	11.282957	-0.051103	4.815533
244.215923	7999.758347	11.287962	-0.051080	4.815505
244.164199	7999.889936	11.292967	-0.051070	4.815544
244.065053	7999.797574	11.297971	-0.051052	4.815517
244.246032	7999.844322	11.302976	-0.051086	4.815530
244.121929	7999.854066	11.307981	-0.051063	4.815533
244.326518	7999.809364	11.312986	-0.051101	4.815519
244.295384	7999.881490	11.317991	-0.051096	4.815541
244.140844	7999.837346	11.322995	-0.051067	4.815528
244.319943	7999.852028	11.328000	-0.051101	4.815532
244.309700	7999.951190	11.333005	-0.051099	4.815561
244.424417	7999.722423	11.338010	-0.051121	4.815493
244.319274	7999.831786	11.343015	-0.051101	4.815526
244.369923	7999.898836	11.348019	-0.051111	4.815545
244.265958	7999.881144	11.353024	-0.051092	4.815541
244.026103	7999.885799	11.358029	-0.051047	4.815543
244.298189	7999.778126	11.363034	-0.051098	4.815510
244.482008	7999.829193	11.368039	-0.051133	4.815524
244.199212	7999.864116	11.373043	-0.051080	4.815536
244.208586	7999.815167	11.378048	-0.051082	4.815522
244.272819	7999.848267	11.383053	-0.051094	4.815531
244.483115	7999.774827	11.388058	-0.051134	4.815508
244.165556	7999.809184	11.393063	-0.051075	4.815520
244.440274	7999.877748	11.398067	-0.051126	4.815539
244.564622	7999.794365	11.403072	-0.051150	4.815514
244.450467	7999.843781	11.408077	-0.051129	4.815529
244.268790	7999.835502	11.413082	-0.051095	4.815527
244.287969	7999.866801	11.418087	-0.051099	4.815536
244.453828	7999.824672	11.423091	-0.051130	4.815523
244.319321	7999.768040	11.428096	-0.051105	4.815507
244.368170	7999.900200	11.433101	-0.051114	4.815546
244.552719	7999.900022	11.438106	-0.051149	4.815545
244.436433	7999.802040	11.443111	-0.051127	4.815517
244.217733	7999.750445	11.448115	-0.051087	4.815503
244.509169	7999.818213	11.453120	-0.051141	4.815521
244.138753	8000.148572	11.458125	-0.051073	4.815619
244.353693	8000.080547	11.463130	-0.051113	4.815598
244.488355	7999.962092	11.468135	-0.051138	4.815563
244.615195	7999.840306	11.473139	-0.051162	4.815527
244.640170	7999.749965	11.478144	-0.051167	4.815500
244.464501	7999.926521	11.483149	-0.051134	4.815553
244.583168	7999.789653	11.488154	-0.051157	4.815512
244.540934	7999.904312	11.493159	-0.051149	4.815546
244.578683	7999.847282	11.498163	-0.051156	4.815529
244.615720	7999.798783	11.503168	-0.051163	4.815515
244.556485	7999.860840	11.508173	-0.051153	4.815533
244.407244	7999.852021	11.513178	-0.051125	4.815531
244.364969	7999.806502	11.518183	-0.051117	4.815518
244.457839	7999.831527	11.523187	-0.051135	4.815525
244.340443	7999.878754	11.528192	-0.051113	4.815539
244.406447	7999.840338	11.533197	-0.051126	4.815528
244.511248	7999.795079	11.538202	-0.051146	4.815514
244.536247	7999.915105	11.543207	-0.051150	4.815549
244.601479	7999.752805	11.548211	-0.051163	4.815501
244.599487	7999.844627	11.553216	-0.051163	4.815528
244.488071	7999.822542	11.558221	-0.051142	4.815522
244.464370	7999.867025	11.563226	-0.051138	4.815535
244.618803	7999.848203	11.568231	-0.051167	4.815529
244.602152	7999.816983	11.573235	-0.051164	4.815520
244.600849	7999.884255	11.578240	-0.051164	4.815540
244.598419	7999.846860	11.583245	-0.051164	4.815529
244.622088	7999.845129	11.588250	-0.051168	4.815528
244.388255	7999.873374	11.593255	-0.051125	4.815537
244.375941	7999.830479	11.598259	-0.051123	4.815525
244.558057	7999.859093	11.603264	-0.051157	4.815532
244.405964	7999.841685	11.608269	-0.051129	4.815528
244.268423	7999.828785	11.613274	-0.051104	4.815525
244.541086	7999.907995	11.618279	-0.051155	4.815547
244.443135	7999.878654	11.623283	-0.051137	4.815539
244.703523	7999.760112	11.628288	-0.051185	4.815503
244.502548	7999.951207	11.633293	-0.051148	4.815560
244.560812	7999.841118	11.638298	-0.051159	4.815527
244.582307	7999.839352	11.643303	-0.051163	4.815527
244.484970	7999.874092	11.648307	-0.051145	4.815537
244.706684	7999.794431	11.653312	-0.051187	4.815513
244.803556	7999.888932	11.658317	-0.051205	4.815540
244.562262	7999.757945	11.663322	-0.051160	4.815503
244.718669	7999.983694	11.668327	-0.051190	4.815568
244.636289	7999.839278	11.673331	-0.051175	4.815526
244.529704	7999.754268	11.678336	-0.051155	4.815502
244.388106	7999.837409	11.683341	-0.051129	4.815527
244.763570	7999.857427	11.688346	-0.051199	4.815531
244.741720	7999.784476	11.693351	-0.051195	4.815510
244.678102	7999.856073	11.698355	-0.051184	4.815531
244.819328	7999.770828	11.703360	-0.051210	4.815505
244.907937	7999.868398	11.708365	-0.051227	4.815533
244.577586	7999.867306	11.713370	-0.051166	4.815535
244.523305	7999.786352	11.718375	-0.051156	4.815511
244.573276	7999.837375	11.723379	-0.051165	4.815526
244.600861	7999.832504	11.728384	-0.051171	4.815524
244.573031	7999.896141	11.733389	-0.051166	4.815543
244.850675	7999.802440	11.738394	-0.051217	4.815514
244.701270	7999.818179	11.743399	-0.051190	4.815520
244.493854	7999.866076	11.748403	-0.051151	4.815535
244.578858	7999.848259	11.753408	-0.051168	4.815529
244.865798	7999.815577	11.758413	-0.051221	4.815518
244.651878	7999.768329	11.763418	-0.051182	4.815505
244.704855	7999.866386	11.768423	-0.051192	4.815534
244.666790	7999.875396	11.773427	-0.051185	4.815537
244.751498	7999.859710	11.778432	-0.051201	4.815532
244.496676	7999.761606	11.783437	-0.051153	4.815504
244.631077	7999.859922	11.788442	-0.051179	4.815532
244.682848	7999.853309	11.793447	-0.051189	4.815530
244.630839	7999.916552	11.798451	-0.051179	4.815549
244.746444	7999.815941	11.803456	-0.051201	4.815519
244.853428	7999.865756	11.808461	-0.051221	4.815533
244.751603	7999.820334	11.813466	-0.051202	4.815520
244.650853	7999.827255	11.818471	-0.051184	4.815523
244.676446	7999.852252	11.823475	-0.051189	4.815530
244.821138	7999.802303	11.828480	-0.051216	4.815514
244.604268	7999.834028	11.833485	-0.051176	4.815525
244.768076	7999.853802	11.838490	-0.051206	4.815530
244.695806	7999.882543	11.843495	-0.051193	4.815538
244.492690	7999.936918	11.848499	-0.051156	4.815555
244.756277	7999.772510	11.853504	-0.051205	4.815506
244.667484	7999.746522	11.858509	-0.051189	4.815499
244.623656	7999.845137	11.863514	-0.051181	4.815528
244.502087	7999.894433	11.868519	-0.051158	4.815543
244.732738	7999.843749	11.873523	-0.051201	4.815527
244.894319	7999.885912	11.878528	-0.051232	4.815538
244.728416	7999.764695	11.883533	-0.051201	4.815504
244.864265	7999.898275	11.888538	-0.051227	4.815542
244.845208	7999.895847	11.893543	-0.051223	4.815542
244.767818	7999.860434	11.898547	-0.051209	4.815532
244.690917	7999.774839	11.903552	-0.051195	4.815507
244.832485	7999.906376	11.908557	-0.051222	4.815545
244.828962	7999.821977	11.913562	-0.051221	4.815520
244.760146	7999.866793	11.918567	-0.051208	4.815533
244.693762	7999.785641	11.923571	-0.051196	4.815510
244.867618	7999.801307	11.928576	-0.051229	4.815514
244.670580	7999.885680	11.933581	-0.051192	4.815539
244.503487	7999.752699	11.938586	-0.051162	4.815501
244.618263	7999.904087	11.943591	-0.051183	4.815545
244.431415	7999.861551	11.948595	-0.051149	4.815533
244.581323	7999.765770	11.953600	-0.051177	4.815505
244.608986	7999.835650	11.958605	-0.051182	4.815525
244.695955	7999.802915	11.963610	-0.051198	4.815515
244.645072	7999.933452	11.968615	-0.051189	4.815553
244.790426	7999.844003	11.973619	-0.051217	4.815527
244.812685	7999.818756	11.978624	-0.051221	4.815519
244.681217	7999.821973	11.983629	-0.051197	4.815521
244.692096	7999.911869	11.988634	-0.051199	4.815547
244.781148	7999.830046	11.993639	-0.051216	4.815523
244.890677	7999.886311	11.998643	-0.051236	4.815538
244.790850	7999.793935	12.003648	-0.051218	4.815512
244.890001	7999.821198	12.008653	-0.051237	4.815519
244.750816	7999.836035	12.013658	-0.051211	4.815524
244.769961	7999.817145	12.018663	-0.051215	4.815519
244.636256	7999.853429	12.023667	-0.051190	4.815530
244.828139	7999.778620	12.028672	-0.051226	4.815507
244.655531	7999.866595	12.033677	-0.051194	4.815534
244.804414	7999.839140	12.038682	-0.051222	4.815525
244.865452	7999.879665	12.043687	-0.051234	4.815537
244.754892	7999.770028	12.048691	-0.051213	4.815505
244.799590	7999.778251	12.053696	-0.051222	4.815507
244.793812	7999.859333	12.058701	-0.051221	4.815531
244.718180	7999.800455	12.063706	-0.051207	4.815514
244.761138	7999.849228	12.068711	-0.051215	4.815528
244.712606	7999.817489	12.073715	-0.051206	4.815519
244.848428	7999.868842	12.078720	-0.051232	4.815533
244.833701	7999.871825	12.083725	-0.051229	4.815534
244.620858	7999.853426	12.088730	-0.051190	4.815530
244.877942	7999.877923	12.093735	-0.051238	4.815536
244.526982	7999.851935	12.098739	-0.051173	4.815530
244.430325	7999.759612	12.103744	-0.051155	4.815503
244.389401	7999.859342	12.108749	-0.051148	4.815533
244.555818	7999.822562	12.113754	-0.051179	4.815521
244.549137	7999.854508	12.118759	-0.051178	4.815531
244.597805	7999.776299	12.123763	-0.051187	4.815508
245.011422	7999.793735	12.128768	-0.051264	4.815511
244.684695	7999.902692	12.133773	-0.051204	4.815544
244.658605	7999.828603	12.138778	-0.051199	4.815523
244.998097	7999.856579	12.143783	-0.051263	4.815529
244.932806	7999.859806	12.148787	-0.051251	4.815530
244.975760	7999.804996	12.153792	-0.051259	4.815514
244.891664	7999.874124	12.158797	-0.051243	4.815535
245.152508	7999.857036	12.163802	-0.051292	4.815528
244.966457	7999.818784	12.168807	-0.051258	4.815518
244.833118	7999.884974	12.173811	-0.051233	4.815538
244.918754	7999.783873	12.178816	-0.051249	4.815508
244.877610	7999.841954	12.183821	-0.051242	4.815525
244.557607	7999.781231	12.188826	-0.051183	4.815509
244.715902	7999.863919	12.193831	-0.051212	4.815532
244.558593	7999.862443	12.198835	-0.051183	4.815533
244.751891	7999.727857	12.203840	-0.051219	4.815493
244.738597	7999.875024	12.208845	-0.051217	4.815536
244.855711	7999.807541	12.213850	-0.051239	4.815515
244.818189	7999.930821	12.218855	-0.051232	4.815552
244.665995	7999.822641	12.223859	-0.051204	4.815521
244.819998	7999.807016	12.228864	-0.051233	4.815515
244.793485	7999.763889	12.233869	-0.051228	4.815503
244.684480	7999.839018	12.238874	-0.051208	4.815525
244.767549	7999.872426	12.243879	-0.051224	4.815535
244.668022	7999.829177	12.248883	-0.051206	4.815523
244.940974	7999.773843	12.253888	-0.051257	4.815505
244.647363	7999.927122	12.258893	-0.051202	4.815551
244.738612	7999.779127	12.263898	-0.051219	4.815508
244.937221	7999.871015	12.268903	-0.051257	4.815533
244.856040	7999.796029	12.273907	-0.051242	4.815512
244.862468	7999.780135	12.278912	-0.051243	4.815507
244.701379	7999.855483	12.283917	-0.051213	4.815530
244.679698	7999.764381	12.288922	-0.051210	4.815503
244.826363	7999.929105	12.293927	-0.051237	4.815551
244.795206	7999.738536	12.298931	-0.051232	4.815495
244.770374	7999.806494	12.303936	-0.051227	4.815515
244.814938	7999.905483	12.308941	-0.051236	4.815544
244.805977	7999.750516	12.313946	-0.051234	4.815499
244.772931	7999.859986	12.318951	-0.051228	4.815531
244.783435	7999.839887	12.323955	-0.051230	4.815525
244.954840	7999.747659	12.328960	-0.051263	4.815497
244.821307	7999.914225	12.333965	-0.051238	4.815547
244.730110	7999.848686	12.338970	-0.051221	4.815528
244.760808	7999.807559	12.343975	-0.051227	4.815516
244.733754	7999.851987	12.348979	-0.051222	4.815529
244.734554	7999.879784	12.353984	-0.051223	4.815537
244.537066	7999.875517	12.358989	-0.051186	4.815537
244.748739	7999.820253	12.363994	-0.051226	4.815519
244.877731	7999.824509	12.368999	-0.051250	4.815520
244.680412	7999.936643	12.374003	-0.051214	4.815554
244.841847	7999.796198	12.379008	-0.051244	4.815512
244.835761	7999.815340	12.384013	-0.051243	4.815518
244.787468	7999.849812	12.389018	-0.051234	4.815528
244.872334	7999.871503	12.394023	-0.051250	4.815534
244.920654	7999.772998	12.399027	-0.051259	4.815505
244.818542	7999.794846	12.404032	-0.051240	4.815512
244.749105	7999.867417	12.409037	-0.051228	4.815533
244.954004	7999.891064	12.414042	-0.051266	4.815539
245.029858	7999.897659	12.419047	-0.051281	4.815541
244.997612	7999.838419	12.424051	-0.051275	4.815523
244.896772	7999.833592	12.429056	-0.051256	4.815523
245.088390	7999.752372	12.434061	-0.051292	4.815498
244.986387	7999.974982	12.439066	-0.051273	4.815563
244.971224	7999.825251	12.444071	-0.051271	4.815520
244.817950	7999.898592	12.449075	-0.051242	4.815542
244.904043	7999.824195	12.454080	-0.051259	4.815520
244.955874	7999.867773	12.459085	-0.051269	4.815532
244.972545	7999.739920	12.464090	-0.051272	4.815495
245.135968	7999.914529	12.469095	-0.051303	4.815545
245.113127	7999.833018	12.474099	-0.051298	4.815521
245.133256	7999.794922	12.479104	-0.051302	4.815510
245.030691	7999.811423	12.484109	-0.051284	4.815515
244.959846	7999.836985	12.489114	-0.051271	4.815523
245.127131	7999.858951	12.494119	-0.051302	4.815529
245.126699	7999.797027	12.499123	-0.051302	4.815511
245.105079	7999.928042	12.504128	-0.051298	4.815549
244.910993	7999.805297	12.509133	-0.051262	4.815514
244.983273	7999.844937	12.514138	-0.051276	4.815525
245.172765	7999.876877	12.519143	-0.051312	4.815534
245.080188	7999.771803	12.524147	-0.051294	4.815503
244.958169	7999.792260	12.529152	-0.051272	4.815510
245.134762	7999.886993	12.534157	-0.051305	4.815537
244.932027	7999.892251	12.539162	-0.051268	4.815539
244.851168	7999.837560	12.544167	-0.051253	4.815524
245.010671	7999.769698	12.549171	-0.051283	4.815503
244.967928	7999.775428	12.554176	-0.051275	4.815505
245.026654	7999.870377	12.559181	-0.051286	4.815532
244.888576	7999.763495	12.564186	-0.051261	4.815502
245.180936	7999.859047	12.569191	-0.051315	4.815528
244.905117	7999.944272	12.574195	-0.051264	4.815555
245.254494	7999.744954	12.579200	-0.051329	4.815495
245.236134	7999.940095	12.584205	-0.051326	4.815552
245.112057	7999.770435	12.589210	-0.051303	4.815503
245.089546	7999.879011	12.594215	-0.051299	4.815535
245.053157	7999.753496	12.599219	-0.051293	4.815498
245.269141	7999.828582	12.604224	-0.051333	4.815519
245.131174	7999.959837	12.609229	-0.051308	4.815558
245.030763	7999.749985	12.614234	-0.051289	4.815497
245.102553	7999.854757	12.619239	-0.051303	4.815528
244.932718	7999.816769	12.624243	-0.051271	4.815517
244.913133	7999.792976	12.629248	-0.051268	4.815510
245.011131	7999.909922	12.634253	-0.051286	4.815544
244.967265	7999.847289	12.639258	-0.051278	4.815526
244.934196	7999.806191	12.644263	-0.051273	4.815514
244.860945	7999.830645	12.649267	-0.051259	4.815522
245.126636	7999.888387	12.654272	-0.051309	4.815537
245.042221	7999.779176	12.659277	-0.051293	4.815506
244.905944	7999.816485	12.664282	-0.051268	4.815517
245.067398	7999.835153	12.669287	-0.051298	4.815522
245.002040	7999.835175	12.674291	-0.051286	4.815522
245.118274	7999.839224	12.679296	-0.051308	4.815523
245.262749	7999.896060	12.684301	-0.051336	4.815539
245.190494	7999.868204	12.689306	-0.051322	4.815531
245.100641	7999.800551	12.694311	-0.051306	4.815512
245.030320	7999.870971	12.699315	-0.051293	4.815532
245.147034	7999.828042	12.704320	-0.051315	4.815519
245.059307	7999.878957	12.709325	-0.051299	4.815535
244.986879	7999.840420	12.714330	-0.051285	4.815524
245.135728	7999.792675	12.719335	-0.051313	4.815509
245.100976	7999.843386	12.724339	-0.051307	4.815524
245.016377	7999.771547	12.729344	-0.051292	4.815503
244.948475	7999.869771	12.734349	-0.051279	4.815532
245.034706	7999.845567	12.739354	-0.051295	4.815525
244.849048	7999.777421	12.744359	-0.051261	4.815506
244.833502	7999.917077	12.749363	-0.051258	4.815547
244.748735	7999.855914	12.754368	-0.051243	4.815529
244.913381	7999.920553	12.759373	-0.051274	4.815547
244.776935	7999.781662	12.764378	-0.051248	4.815508
245.118347	7999.829958	12.769383	-0.051312	4.815520
244.848896	7999.846944	12.774387	-0.051262	4.815526
244.781827	7999.759374	12.779392	-0.051250	4.815501
244.868819	7999.787507	12.784397	-0.051266	4.815509
245.028978	7999.906533	12.789402	-0.051297	4.815543
244.960031	7999.884071	12.794407	-0.051284	4.815537
244.948724	7999.852938	12.799411	-0.051282	4.815528
244.994597	7999.809922	12.804416	-0.051291	4.815515
245.030289	8000.086035	12.809421	-0.051298	4.815595
244.947517	7999.941609	12.814426	-0.051283	4.815553
245.022026	7999.830716	12.819431	-0.051297	4.815521
244.940378	7999.934056	12.824435	-0.051282	4.815551
245.128904	7999.860260	12.829440	-0.051317	4.815529
245.081536	7999.937462	12.834445	-0.051308	4.815552
244.909092	7999.858852	12.839450	-0.051276	4.815529
245.130544	7999.898788	12.844455	-0.051318	4.815540
245.030119	7999.865134	12.849459	-0.051299	4.815531
245.022169	7999.735811	12.854464	-0.051298	4.815493
244.992720	7999.940382	12.859469	-0.051293	4.815553
244.959748	7999.834144	12.864474	-0.051287	4.815522
245.079283	7999.800871	12.869479	-0.051309	4.815512
244.918744	7999.876229	12.874483	-0.051280	4.815534
244.957679	7999.839507	12.879488	-0.051287	4.815523
245.182035	7999.783381	12.884493	-0.051329	4.815506
244.923558	7999.936166	12.889498	-0.051281	4.815552
244.877203	7999.836117	12.894503	-0.051273	4.815523
244.893343	7999.882318	12.899507	-0.051276	4.815536
244.964515	7999.841850	12.904512	-0.051290	4.815524
245.122785	7999.864738	12.909517	-0.051319	4.815530
244.838080	7999.816335	12.914522	-0.051266	4.815517
244.979194	7999.852825	12.919527	-0.051293	4.815527
244.881599	7999.908919	12.924531	-0.051275	4.815544
245.072262	7999.890688	12.929536	-0.051311	4.815538
245.189106	7999.832810	12.934541	-0.051333	4.815520
245.097461	7999.872983	12.939546	-0.051316	4.815532
245.221558	7999.778915	12.944551	-0.051339	4.815504
244.940511	7999.898228	12.949555	-0.051287	4.815541
245.114385	7999.751578	12.954560	-0.051320	4.815497
245.233430	7999.888090	12.959565	-0.051342	4.815536
245.167593	7999.845389	12.964570	-0.051330	4.815524
245.068093	7999.899316	12.969575	-0.051312	4.815540
244.870829	7999.838455	12.974579	-0.051275	4.815523
245.353920	7999.752374	12.979584	-0.051365	4.815496
244.798158	7999.864006	12.984589	-0.051262	4.815531
244.855131	7999.853207	12.989594	-0.051273	4.815528
245.011465	7999.807719	12.994599	-0.051302	4.815514
244.843108	7999.856252	12.999603	-0.051271	4.815529
244.974451	7999.772982	13.004608	-0.051296	4.815504
244.948395	7999.831310	13.009613	-0.051291	4.815521
244.916543	7999.801977	13.014618	-0.051285	4.815513
245.086732	7999.929711	13.019623	-0.051317	4.815549
244.919583	7999.805269	13.024627	-0.051286	4.815513
245.097388	7999.778285	13.029632	-0.051320	4.815505
245.076695	7999.898636	13.034637	-0.051316	4.815540
244.876651	7999.816373	13.039642	-0.051279	4.815517
245.156215	7999.795319	13.044647	-0.051331	4.815509
245.014071	7999.862433	13.049651	-0.051305	4.815530
245.379815	7999.852395	13.054656	-0.051373	4.815525
245.230192	7999.795514	13.059661	-0.051346	4.815509
245.108223	7999.861889	13.064666	-0.051323	4.815529
245.182711	7999.817203	13.069671	-0.051337	4.815516
245.277718	7999.912744	13.074675	-0.051355	4.815543
245.145299	7999.738677	13.079680	-0.051331	4.815493
245.163064	7999.882081	13.084685	-0.051334	4.815535
245.088697	7999.776237	13.089690	-0.051321	4.815504
245.315363	7999.823732	13.094695	-0.051363	4.815517
245.095414	7999.912004	13.099699	-0.051322	4.815544
245.126946	7999.797207	13.104704	-0.051328	4.815510
245.054720	7999.805660	13.109709	-0.051315	4.815513
245.164095	7999.823479	13.114714	-0.051336	4.815518
245.212461	7999.891563	13.119719	-0.051345	4.815537
245.223436	7999.804195	13.124723	-0.051347	4.815512
245.211680	7999.804022	13.129728	-0.051345	4.815512
245.174858	7999.892075	13.134733	-0.051339	4.815537
245.107868	7999.871781	13.139738	-0.051327	4.815532
245.396174	7999.778254	13.144743	-0.051380	4.815503
245.336400	7999.971654	13.149747	-0.051370	4.815560
245.224886	7999.745600	13.154752	-0.051349	4.815494
245.224328	7999.884434	13.159757	-0.051349	4.815535
245.100112	7999.851460	13.164762	-0.051326	4.815526
245.042074	7999.796072	13.169767	-0.051316	4.815510
245.062372	7999.896802	13.174771	-0.051320	4.815539
245.181503	7999.814400	13.179776	-0.051342	4.815515
245.224824	7999.834347	13.184781	-0.051350	4.815520
245.093555	7999.885621	13.189786	-0.051326	4.815536
245.061279	7999.790073	13.194791	-0.051320	4.815508
244.936409	7999.846790	13.199795	-0.051297	4.815525
245.092346	7999.757514	13.204800	-0.051326	4.815498
245.263860	7999.888473	13.209805	-0.051359	4.815536
245.215683	7999.882368	13.214810	-0.051350	4.815534
245.185541	7999.828501	13.219815	-0.051344	4.815519
245.156005	7999.818428	13.224819	-0.051339	4.815516
245.152078	7999.871777	13.229824	-0.051339	4.815532
244.961230	7999.916741	13.234829	-0.051303	4.815546
244.870314	7999.763640	13.239834	-0.051287	4.815501
245.156222	7999.883649	13.244839	-0.051340	4.815535
245.267681	7999.822480	13.249843	-0.051361	4.815517
245.174898	7999.843412	13.254848	-0.051344	4.815523
245.242051	7999.858408	13.259853	-0.051357	4.815527
245.081995	7999.825918	13.264858	-0.051327	4.815518
245.160555	7999.875272	13.269863	-0.051342	4.815532
245.070672	7999.778785	13.274867	-0.051325	4.815505
245.233458	7999.783593	13.279872	-0.051356	4.815505
245.313785	7999.911999	13.284877	-0.051371	4.815542
245.281752	7999.844219	13.289882	-0.051365	4.815523
245.298184	7999.762280	13.294887	-0.051369	4.815499
245.032113	7999.846596	13.299891	-0.051319	4.815525
245.215060	7999.877362	13.304896	-0.051354	4.815533
245.286606	7999.819814	13.309901	-0.051367	4.815516
245.402215	7999.822785	13.314906	-0.051389	4.815516
245.380374	7999.837398	13.319911	-0.051385	4.815520
245.219782	7999.830529	13.324915	-0.051355	4.815519
245.381008	7999.824632	13.329920	-0.051386	4.815517
245.394903	7999.861186	13.334925	-0.051388	4.815527
245.061509	7999.846160	13.339930	-0.051327	4.815524
245.333589	7999.815374	13.344935	-0.051377	4.815514
245.239736	7999.850171	13.349939	-0.051360	4.815525
245.002089	7999.897575	13.354944	-0.051316	4.815540
245.156383	7999.821086	13.359949	-0.051345	4.815517
245.189843	7999.866501	13.364954	-0.051352	4.815530
245.179839	7999.979553	13.369959	-0.051350	4.815563
245.257654	8000.002199	13.374963	-0.051365	4.815569
245.563935	7999.885471	13.379968	-0.051422	4.815533
245.501173	7999.824665	13.384973	-0.051410	4.815516
245.311058	7999.862165	13.389978	-0.051375	4.815528
245.354488	7999.828720	13.394983	-0.051384	4.815518
245.252278	7999.893282	13.399987	-0.051365	4.815537
245.264088	7999.769620	13.404992	-0.051367	4.815501
245.242756	7999.878215	13.409997	-0.051363	4.815533
245.525849	7999.859355	13.415002	-0.051416	4.815526
245.552355	7999.833109	13.420007	-0.051421	4.815518
245.459143	7999.924515	13.425011	-0.051404	4.815545
245.380098	7999.860240	13.430016	-0.051390	4.815527
245.662050	7999.793306	13.435021	-0.051443	4.815506
245.413318	7999.923825	13.440026	-0.051397	4.815545
245.560924	7999.797036	13.445031	-0.051424	4.815508
245.621108	7999.782018	13.450035	-0.051436	4.815503
245.464608	7999.848898	13.455040	-0.051407	4.815523
245.603944	7999.854392	13.460045	-0.051433	4.815524
245.569626	7999.953166	13.465050	-0.051427	4.815553
245.787058	7999.809360	13.470055	-0.051467	4.815510
245.476505	7999.885477	13.475059	-0.051410	4.815534
245.465149	7999.756097	13.480064	-0.051408	4.815496
245.545831	7999.895188	13.485069	-0.051423	4.815536
245.278495	7999.847066	13.490074	-0.051374	4.815523
245.496748	7999.888019	13.495079	-0.051414	4.815534
245.423699	7999.892187	13.500083	-0.051401	4.815536
245.281033	7999.890948	13.505088	-0.051375	4.815536
245.457595	7999.859673	13.510093	-0.051408	4.815526
245.498854	7999.832600	13.515098	-0.051416	4.815518
245.447268	7999.849932	13.520103	-0.051406	4.815523
245.187915	7999.938630	13.525107	-0.051358	4.815551
245.339840	7999.842880	13.530112	-0.051387	4.815522
245.585570	7999.885348	13.535117	-0.051433	4.815533
245.490006	7999.825076	13.540122	-0.051415	4.815516
245.425164	7999.857142	13.545127	-0.051403	4.815526
245.556032	7999.887060	13.550131	-0.051428	4.815534
245.480340	7999.867691	13.555136	-0.051414	4.815528
245.581380	7999.811691	13.560141	-0.051433	4.815512
245.459183	7999.868452	13.565146	-0.051410	4.815529
245.551148	7999.875310	13.570151	-0.051428	4.815530
245.238947	7999.770927	13.575155	-0.051370	4.815501
245.525144	7999.943269	13.580160	-0.051423	4.815550
245.604736	7999.780131	13.585165	-0.051438	4.815502
245.488010	7999.942702	13.590170	-0.051417	4.815550
245.572800	7999.828771	13.595175	-0.051433	4.815517
245.515690	7999.822520	13.600179	-0.051422	4.815515
245.431833	7999.785932	13.605184	-0.051407	4.815505
245.586364	7999.926228	13.610189	-0.051436	4.815545
245.513262	7999.855642	13.615194	-0.051423	4.815525
245.490765	7999.817919	13.620199	-0.051419	4.815514
245.462049	7999.910376	13.625203	-0.051414	4.815541
245.697056	7999.775400	13.630208	-0.051458	4.815500
245.769022	7999.897265	13.635213	-0.051471	4.815536
245.502539	7999.897211	13.640218	-0.051422	4.815537
245.667155	7999.843315	13.645223	-0.051453	4.815520
245.786867	8000.028965	13.650227	-0.051475	4.815574
245.659942	7999.857118	13.655232	-0.051452	4.815524
245.459976	7999.857082	13.660237	-0.051415	4.815525
245.354043	7999.840424	13.665242	-0.051395	4.815521
245.509053	7999.896364	13.670247	-0.051424	4.815537
245.435685	7999.871693	13.675251	-0.051411	4.815530
245.358366	7999.808515	13.680256	-0.051397	4.815512
245.489364	7999.838434	13.685261	-0.051421	4.815520
245.561810	7999.973121	13.690266	-0.051435	4.815559
245.494149	7999.770206	13.695271	-0.051423	4.815500
245.519462	7999.867815	13.700275	-0.051428	4.815528
245.417312	7999.975094	13.705280	-0.051409	4.815560
245.458286	7999.864720	13.710285	-0.051417	4.815528
245.570116	7999.869766	13.715290	-0.051438	4.815528
245.620076	7999.849242	13.720295	-0.051447	4.815522
245.491763	7999.916582	13.725299	-0.051424	4.815542
245.652274	7999.905335	13.730304	-0.051454	4.815538
245.900944	7999.833588	13.735309	-0.051500	4.815516
245.548499	7999.917564	13.740314	-0.051435	4.815542
245.700323	7999.798319	13.745319	-0.051463	4.815507
245.644786	7999.986450	13.750323	-0.051453	4.815562
245.609441	7999.869492	13.755328	-0.051447	4.815528
245.600088	7999.804217	13.760333	-0.051445	4.815509
245.463635	7999.891715	13.765338	-0.051420	4.815535
245.619636	7999.821661	13.770343	-0.051449	4.815514
245.861836	7999.854461	13.775347	-0.051495	4.815523
245.739245	7999.911216	13.780352	-0.051472	4.815540
245.700458	7999.887109	13.785357	-0.051465	4.815533
245.709847	7999.841362	13.790362	-0.051467	4.815519
245.677126	7999.842983	13.795367	-0.051461	4.815520
245.617464	7999.877270	13.800371	-0.051450	4.815530
245.671428	7999.835453	13.805376	-0.051460	4.815518
245.758446	7999.893489	13.810381	-0.051477	4.815534
245.689098	7999.955384	13.815386	-0.051464	4.815553
245.688943	7999.859290	13.820391	-0.051464	4.815525
245.626025	7999.835857	13.825395	-0.051453	4.815518
245.552306	7999.791959	13.830400	-0.051439	4.815506
245.540356	7999.959443	13.835405	-0.051437	4.815555
245.665519	7999.822676	13.840410	-0.051461	4.815514
245.650313	7999.827787	13.845415	-0.051458	4.815516
245.532340	7999.852580	13.850419	-0.051437	4.815523
245.768545	7999.906641	13.855424	-0.051481	4.815538
245.711738	7999.806420	13.860429	-0.051470	4.815509
245.502548	7999.814776	13.865434	-0.051432	4.815513
245.702219	7999.902413	13.870439	-0.051469	4.815537
245.725339	7999.900673	13.875443	-0.051474	4.815537
245.819856	7999.881944	13.880448	-0.051491	4.815531
245.746830	7999.879704	13.885453	-0.051478	4.815530
245.706369	7999.802175	13.890458	-0.051471	4.815508
245.703775	7999.834189	13.895463	-0.051470	4.815517
245.661107	7999.923216	13.900467	-0.051463	4.815543
245.667123	7999.785574	13.905472	-0.051464	4.815503
245.521001	7999.926309	13.910477	-0.051437	4.815545
245.527743	7999.813242	13.915482	-0.051438	4.815512
245.737793	7999.914931	13.920487	-0.051478	4.815541
245.752121	7999.790240	13.925491	-0.051481	4.815504
245.632165	7999.895093	13.930496	-0.051459	4.815535
245.699710	7999.850294	13.935501	-0.051471	4.815522
245.712149	7999.838769	13.940506	-0.051474	4.815518
245.622585	7999.815970	13.945511	-0.051457	4.815512
245.569461	7999.838617	13.950515	-0.051448	4.815519
245.625749	7999.888677	13.955520	-0.051459	4.815533
245.726943	7999.856173	13.960525	-0.051478	4.815523
245.708762	7999.902883	13.965530	-0.051474	4.815537
245.643283	7999.787570	13.970535	-0.051462	4.815504
245.737097	7999.894840	13.975539	-0.051480	4.815535
245.773547	7999.886910	13.980544	-0.051487	4.815532
245.713862	7999.815475	13.985549	-0.051476	4.815512
245.747461	7999.903610	13.990554	-0.051483	4.815537
245.747762	7999.789369	13.995559	-0.051483	4.815504
245.513783	7999.881684	14.000563	-0.051440	4.815532
245.769149	7999.880527	14.005568	-0.051487	4.815530
245.791632	7999.806160	14.010573	-0.051492	4.815508
245.625947	7999.892113	14.015578	-0.051461	4.815534
245.832422	7999.825017	14.020583	-0.051500	4.815514
245.884460	7999.936946	14.025587	-0.051510	4.815546
245.663477	7999.781721	14.030592	-0.051469	4.815502
245.666226	7999.828772	14.035597	-0.051470	4.815516
245.640280	7999.945837	14.040602	-0.051465	4.815550
245.651621	7999.776246	14.045607	-0.051467	4.815500
245.676175	7999.911220	14.050611	-0.051472	4.815540
245.696813	7999.772749	14.055616	-0.051476	4.815499
245.845775	7999.932178	14.060621	-0.051504	4.815545
245.701010	7999.879645	14.065626	-0.051477	4.815530
245.643656	7999.748446	14.070631	-0.051467	4.815492
245.731052	7999.878037	14.075635	-0.051483	4.815530
245.658138	7999.836288	14.080640	-0.051470	4.815518
245.591841	7999.895028	14.085645	-0.051458	4.815535
245.708467	7999.764530	14.090650	-0.051480	4.815497
245.995760	7999.900584	14.095655	-0.051534	4.815535
245.714716	7999.846898	14.100659	-0.051481	4.815521
245.671052	7999.876106	14.105664	-0.051474	4.815529
245.880281	7999.815462	14.110669	-0.051513	4.815511
245.676147	7999.853801	14.115674	-0.051475	4.815523
245.542516	7999.891154	14.120679	-0.051450	4.815534
245.980384	7999.888701	14.125683	-0.051532	4.815532
245.774450	7999.872548	14.130688	-0.051494	4.815528
245.639004	7999.904531	14.135693	-0.051469	4.815538
245.626615	7999.778337	14.140698	-0.051467	4.815501
245.893044	7999.917255	14.145703	-0.051517	4.815540
246.018638	7999.844569	14.150707	-0.051540	4.815518
245.860801	7999.851625	14.155712	-0.051511	4.815521
245.866287	7999.932895	14.160717	-0.051512	4.815545
245.682238	7999.846617	14.165722	-0.051478	4.815521
245.584953	7999.866408	14.170727	-0.051460	4.815527
245.846127	7999.904858	14.175731	-0.051509	4.815537
245.995628	7999.873141	14.180736	-0.051537	4.815527
245.966159	7999.806470	14.185741	-0.051532	4.815508
245.920785	7999.882638	14.190746	-0.051524	4.815530
245.843253	7999.865375	14.195751	-0.051509	4.815525
245.766203	7999.859866	14.200755	-0.051495	4.815524
245.971436	7999.885657	14.205760	-0.051534	4.815531
246.100847	7999.815169	14.210765	-0.051558	4.815509
245.773034	7999.822658	14.215770	-0.051497	4.815513
245.732042	7999.829485	14.220775	-0.051490	4.815515
245.843876	7999.893265	14.225779	-0.051511	4.815533
245.878541	7999.878899	14.230784	-0.051518	4.815529
246.016574	7999.829909	14.235789	-0.051543	4.815514
245.631607	7999.894133	14.240794	-0.051472	4.815535
245.724350	7999.813436	14.245799	-0.051490	4.815511
245.538542	7999.578696	14.250803	-0.051455	4.815443

245.595783	7996.340028	14.255808	-0.051464	4.814496
245.729959	7990.761392	14.260813	-0.051485	4.812863
245.606322	7983.961038	14.265818	-0.051458	4.810874
245.481084	7976.667642	14.270823	-0.051430	4.808740
245.643110	7969.045179	14.275827	-0.051456	4.806507
245.640798	7961.144550	14.280832	-0.051450	4.804193
245.640395	7953.454351	14.285837	-0.051445	4.801939
245.475696	7945.369366	14.290842	-0.051410	4.799568
245.386800	7937.453397	14.295847	-0.051388	4.797246
245.559689	7929.421780	14.300851	-0.051415	4.794888
245.423372	7921.371536	14.305856	-0.051385	4.792524
245.363197	7913.378456	14.310861	-0.051369	4.790176
245.080828	7905.394707	14.315866	-0.051311	4.787830
245.081173	7897.371139	14.320871	-0.051306	4.785470
245.370228	7889.436085	14.325875	-0.051355	4.783134
245.208782	7881.409699	14.330880	-0.051320	4.780771
245.532326	7873.434039	14.335885	-0.051375	4.778421
245.174809	7865.355862	14.340890	-0.051304	4.776042
245.139701	7857.371746	14.345895	-0.051292	4.773688
244.969624	7849.356023	14.350899	-0.051256	4.771324
244.970017	7841.341183	14.355904	-0.051251	4.768958
245.119990	7833.412496	14.360909	-0.051274	4.766616
244.887686	7825.316115	14.365914	-0.051225	4.764225
244.737201	7817.399099	14.370919	-0.051192	4.761886
244.727792	7809.377925	14.375923	-0.051186	4.759513
244.735387	7801.386275	14.380928	-0.051182	4.757149
244.779808	7793.374769	14.385933	-0.051185	4.754777
244.500527	7785.339417	14.390938	-0.051128	4.752398
244.608277	7777.340868	14.395943	-0.051143	4.750028
244.500535	7769.345021	14.400947	-0.051118	4.747657
244.458108	7761.348643	14.405952	-0.051105	4.745286
244.563037	7753.332569	14.410957	-0.051120	4.742906
244.479682	7745.315422	14.415962	-0.051099	4.740526
244.500903	7737.345409	14.420967	-0.051098	4.738158
244.460207	7729.348322	14.425971	-0.051086	4.735782
244.456028	7721.359821	14.430976	-0.051080	4.733406
244.493489	7713.323276	14.435981	-0.051082	4.731015
244.394511	7705.241303	14.440986	-0.051058	4.728609
244.460611	7697.315885	14.445991	-0.051066	4.726249
244.308413	7689.304503	14.450995	-0.051032	4.723862
244.314034	7681.315343	14.456000	-0.051029	4.721480
244.427901	7673.327991	14.461005	-0.051045	4.719098
244.134490	7665.385222	14.466010	-0.050985	4.716728
244.036059	7657.341501	14.471015	-0.050962	4.714327
244.006320	7649.320223	14.476019	-0.050951	4.711930
244.045088	7641.247176	14.481024	-0.050953	4.709517
244.109819	7633.316228	14.486029	-0.050961	4.707146
243.917400	7625.284120	14.491034	-0.050920	4.704743
243.969138	7617.315266	14.496039	-0.050924	4.702357
244.129607	7609.329302	14.501043	-0.050949	4.699965
243.673227	7601.323454	14.506048	-0.050859	4.697567
243.679170	7593.294674	14.511053	-0.050855	4.695160
243.696121	7585.309627	14.516058	-0.050854	4.692765
243.884327	7577.243376	14.521063	-0.050884	4.690344
243.764802	7569.290642	14.526067	-0.050856	4.687956
243.879929	7561.242569	14.531072	-0.050873	4.685538
243.723233	7553.311348	14.536077	-0.050839	4.683155
243.511947	7545.302988	14.541082	-0.050794	4.680747
243.572084	7537.277403	14.546087	-0.050800	4.678332
243.499291	7529.341348	14.551091	-0.050782	4.675943
243.181901	7521.243465	14.556096	-0.050718	4.673504
243.404845	7513.139954	14.561101	-0.050754	4.671062
243.240097	7505.173500	14.566106	-0.050719	4.668660
243.333737	7497.209180	14.571111	-0.050731	4.666257
243.271497	7489.199717	14.576115	-0.050714	4.663840
243.222377	7481.236865	14.581120	-0.050700	4.661435
243.192184	7473.255488	14.586125	-0.050690	4.659024
243.097202	7465.259461	14.591130	-0.050667	4.656607
243.137718	7457.225749	14.596135	-0.050670	4.654177
243.327915	7449.279184	14.601139	-0.050700	4.651772
243.149319	7441.197498	14.606144	-0.050662	4.649325
243.052056	7433.254298	14.611149	-0.050639	4.646919
242.912279	7425.182312	14.616154	-0.050608	4.644473
242.991609	7417.241722	14.621159	-0.050617	4.642065
243.081358	7409.206492	14.626163	-0.050629	4.639627
242.879199	7401.255129	14.631168	-0.050586	4.637213
242.758122	7393.214607	14.636173	-0.050559	4.634771
242.597894	7385.184485	14.641178	-0.050524	4.632331
242.635219	7377.156854	14.646183	-0.050526	4.629890
242.828077	7369.220822	14.651187	-0.050557	4.627476
242.673695	7361.145006	14.656192	-0.050523	4.625018
242.665221	7353.223285	14.661197	-0.050517	4.622606
242.611443	7345.176616	14.666202	-0.050502	4.620154
242.676359	7337.215163	14.671207	-0.050509	4.617727
242.464367	7329.213857	14.676211	-0.050464	4.615287
242.271085	7321.128914	14.681216	-0.050423	4.612819
242.636068	7313.140200	14.686221	-0.050486	4.610380
242.508478	7305.141530	14.691226	-0.050457	4.607936
242.555271	7297.185840	14.696231	-0.050461	4.605505
242.500916	7289.236473	14.701235	-0.050446	4.603074
242.334441	7281.164973	14.706240	-0.050410	4.600604
242.275306	7273.219061	14.711245	-0.050394	4.598171
242.190158	7265.160245	14.716250	-0.050373	4.595703
242.282803	7257.120777	14.721255	-0.050385	4.593239
242.194238	7249.095095	14.726259	-0.050364	4.590778
241.968574	7241.100492	14.731264	-0.050317	4.588325
242.031892	7233.123842	14.736269	-0.050324	4.585876
241.893746	7225.162091	14.741274	-0.050293	4.583431
241.973167	7217.136027	14.746279	-0.050303	4.580964
241.913941	7209.141048	14.751283	-0.050287	4.578506
241.861337	7201.133127	14.756288	-0.050272	4.576042
242.003710	7193.145142	14.761293	-0.050293	4.573584
241.914704	7185.065916	14.766298	-0.050272	4.571096
241.966581	7177.079760	14.771303	-0.050277	4.568635
241.786383	7169.156482	14.776307	-0.050238	4.566192
241.808883	7161.120352	14.781312	-0.050237	4.563713
241.973632	7153.184063	14.786317	-0.050263	4.561264
241.817492	7145.146249	14.791322	-0.050229	4.558781
241.478539	7137.146045	14.796327	-0.050161	4.556309
241.736856	7129.123242	14.801331	-0.050204	4.553829
241.612167	7121.059192	14.806336	-0.050176	4.551335
241.718079	7113.099282	14.811341	-0.050190	4.548872
241.651522	7105.125421	14.816346	-0.050173	4.546402
241.648824	7097.088075	14.821351	-0.050167	4.543912
241.398741	7089.161278	14.826355	-0.050116	4.541455
241.213255	7081.109686	14.831360	-0.050076	4.538957
241.355372	7073.172237	14.836365	-0.050098	4.536494
241.209958	7065.116223	14.841370	-0.050066	4.533992
241.089368	7057.093693	14.846375	-0.050038	4.531500
241.389334	7049.087872	14.851379	-0.050089	4.529012
241.320858	7041.131033	14.856384	-0.050071	4.526537
241.302227	7033.094978	14.861389	-0.050063	4.524036
241.192813	7025.135216	14.866394	-0.050038	4.521558
241.280030	7017.142330	14.871399	-0.050049	4.519068
241.179456	7009.194316	14.876403	-0.050025	4.516590
240.899963	7001.069979	14.881408	-0.049968	4.514056
240.903666	6993.015051	14.886413	-0.049964	4.511542
240.882772	6985.026800	14.891418	-0.049955	4.509048
240.644488	6977.059810	14.896423	-0.049905	4.506559
240.813312	6969.051864	14.901427	-0.049932	4.504056
240.596249	6961.099625	14.906432	-0.049887	4.501569
240.826674	6953.082001	14.911437	-0.049924	4.499060
240.599964	6945.093919	14.916442	-0.049877	4.496559
240.647394	6937.046025	14.921447	-0.049881	4.494038
240.713528	6929.066184	14.926451	-0.049888	4.491537
240.730208	6921.023582	14.931456	-0.049886	4.489014
240.448219	6913.095909	14.936461	-0.049829	4.486526
240.408327	6905.063918	14.941466	-0.049817	4.484004
240.413063	6897.065811	14.946471	-0.049812	4.481491
240.471655	6889.039851	14.951475	-0.049818	4.478969
240.500189	6881.061394	14.956480	-0.049819	4.476460
240.564256	6873.035442	14.961485	-0.049826	4.473934
240.367305	6864.996102	14.966490	-0.049784	4.471402
240.383390	6856.973842	14.971495	-0.049782	4.468875
240.343775	6849.064691	14.976499	-0.049770	4.466382
240.091329	6841.064509	14.981504	-0.049718	4.463858
240.351804	6833.039099	14.986509	-0.049761	4.461326
240.174695	6825.063986	14.991514	-0.049723	4.458807
239.982838	6817.051158	14.996519	-0.049682	4.456275
239.990392	6809.041460	15.001523	-0.049679	4.453743
239.908518	6800.937794	15.006528	-0.049658	4.451179
239.863298	6793.006018	15.011533	-0.049645	4.448669
239.918765	6785.004488	15.016538	-0.049650	4.446136
239.816100	6777.025368	15.021543	-0.049626	4.443607
239.891568	6769.035636	15.026547	-0.049635	4.441074
239.710611	6761.022462	15.031552	-0.049597	4.438532
239.702506	6753.062696	15.036557	-0.049590	4.436006
239.678565	6744.986811	15.041562	-0.049581	4.433441
239.658395	6736.948959	15.046567	-0.049572	4.430887
239.585076	6728.968556	15.051571	-0.049553	4.428349
239.530266	6720.962077	15.056576	-0.049538	4.425802
239.593697	6712.990840	15.061581	-0.049545	4.423265
239.473475	6705.005361	15.066586	-0.049518	4.420721
239.524114	6696.983733	15.071591	-0.049522	4.418165
239.421197	6689.009237	15.076595	-0.049498	4.415622
239.331907	6680.973626	15.081600	-0.049476	4.413058
239.503822	6672.943485	15.086605	-0.049503	4.410495
239.618874	6664.961857	15.091610	-0.049520	4.407947
239.319191	6656.954415	15.096615	-0.049459	4.405386
239.326327	6649.004310	15.101619	-0.049455	4.402844
239.352977	6640.950204	15.106624	-0.049455	4.400267
239.323425	6633.040188	15.111629	-0.049445	4.397734
239.241348	6625.032363	15.116634	-0.049424	4.395169
239.046346	6616.974715	15.121639	-0.049383	4.392585
239.201928	6608.917754	15.126643	-0.049407	4.390002
238.842905	6600.970801	15.131648	-0.049335	4.387449
238.978644	6592.946939	15.136653	-0.049355	4.384874
238.965629	6585.005216	15.141658	-0.049348	4.382322
238.997669	6576.968284	15.146663	-0.049349	4.379739
238.995013	6569.016290	15.151667	-0.049344	4.377181
238.954159	6560.996930	15.156672	-0.049331	4.374600
238.893394	6553.007898	15.161677	-0.049315	4.372026
238.550709	6544.965975	15.166682	-0.049246	4.369433
238.737455	6536.987585	15.171687	-0.049276	4.366862
238.915686	6529.001415	15.176691	-0.049304	4.364286
238.656813	6521.048718	15.181696	-0.049251	4.361718
238.624890	6512.985227	15.186701	-0.049240	4.359113
238.906381	6505.033334	15.191706	-0.049287	4.356545
238.520431	6496.957546	15.196711	-0.049210	4.353931
238.564382	6488.907960	15.201715	-0.049213	4.351326
238.458944	6480.890339	15.206720	-0.049189	4.348730
238.504190	6472.927430	15.211725	-0.049192	4.346150
238.307711	6464.992571	15.216730	-0.049151	4.343577
238.209203	6456.933423	15.221735	-0.049127	4.340962
238.304560	6448.987575	15.226739	-0.049140	4.338384
238.207669	6440.967885	15.231744	-0.049117	4.335779
238.245402	6432.943427	15.236749	-0.049119	4.333172
238.290190	6424.916918	15.241754	-0.049122	4.330562
238.215168	6416.951597	15.246759	-0.049103	4.327971
238.075537	6408.980055	15.251763	-0.049072	4.325375
238.075824	6400.935489	15.256768	-0.049067	4.322754
237.950453	6392.954189	15.261773	-0.049039	4.320152
237.918480	6384.965099	15.266778	-0.049028	4.317547
237.957259	6376.948621	15.271783	-0.049030	4.314931
238.082302	6368.949335	15.276787	-0.049049	4.312320
237.938114	6360.872299	15.281792	-0.049017	4.309680
238.017607	6352.915301	15.286797	-0.049027	4.307079
237.976263	6344.923973	15.291802	-0.049014	4.304465
237.828484	6336.944840	15.296807	-0.048981	4.301852
237.944469	6328.958537	15.301811	-0.048998	4.299238
237.727239	6320.964208	15.306816	-0.048953	4.296616
237.806071	6312.926665	15.311821	-0.048962	4.293981
237.652461	6304.884558	15.316826	-0.048929	4.291341
237.771864	6296.894853	15.321831	-0.048946	4.288719
237.924545	6288.948111	15.326835	-0.048969	4.286109
237.710552	6280.874910	15.331840	-0.048924	4.283454
237.542040	6272.966008	15.336845	-0.048888	4.280851
237.558645	6264.945339	15.341850	-0.048886	4.278211
237.448921	6256.939523	15.346855	-0.048861	4.275574
237.597978	6248.897857	15.351859	-0.048884	4.272925
237.500111	6240.843000	15.356864	-0.048860	4.270268
237.276467	6232.899638	15.361869	-0.048814	4.267646
237.130954	6224.864639	15.366874	-0.048782	4.264992
237.057309	6216.902690	15.371879	-0.048763	4.262361
237.065768	6208.896266	15.376883	-0.048759	4.259714
237.012263	6200.921041	15.381888	-0.048745	4.257076
237.145224	6192.897583	15.386893	-0.048764	4.254421
237.092736	6184.901172	15.391898	-0.048750	4.251773
236.938626	6176.874926	15.396903	-0.048716	4.249112
237.039449	6168.953937	15.401907	-0.048730	4.246486
236.893851	6160.898024	15.406912	-0.048697	4.243812
236.968076	6152.949118	15.411917	-0.048706	4.241173
236.908136	6144.956361	15.416922	-0.048690	4.238517
236.732678	6136.943805	15.421927	-0.048653	4.235852
236.938210	6128.957232	15.426931	-0.048686	4.233197
236.903704	6120.890702	15.431936	-0.048674	4.230512
236.777251	6112.911667	15.436941	-0.048646	4.227854
236.570002	6104.932606	15.441946	-0.048602	4.225192
236.579198	6096.887647	15.446951	-0.048599	4.222510
236.564491	6088.942985	15.451955	-0.048591	4.219858
236.232864	6080.968014	15.456960	-0.048525	4.217192
236.582448	6072.947675	15.461965	-0.048585	4.214516
236.505905	6064.922898	15.466970	-0.048565	4.211832
236.324543	6056.883172	15.471975	-0.048527	4.209141
236.390175	6048.949183	15.476979	-0.048534	4.206486
236.207260	6040.941264	15.481984	-0.048495	4.203801
236.064946	6032.972655	15.486989	-0.048463	4.201129
236.066023	6024.964651	15.491994	-0.048458	4.198443
236.154384	6016.959014	15.496999	-0.048470	4.195757
236.150897	6008.900065	15.502003	-0.048464	4.193051
236.118677	6000.801743	15.507008	-0.048453	4.190329
236.199357	5992.834997	15.512013	-0.048463	4.187651
236.017023	5984.878151	15.517018	-0.048424	4.184972
235.935907	5976.925029	15.522023	-0.048404	4.182293
236.062039	5968.891496	15.527027	-0.048423	4.179588
235.856566	5960.913884	15.532032	-0.048379	4.176896
235.935098	5952.939467	15.537037	-0.048389	4.174207
235.846935	5944.896226	15.542042	-0.048368	4.171490
235.700820	5936.861140	15.547047	-0.048335	4.168775
235.728221	5928.899356	15.552051	-0.048336	4.166084
235.605018	5920.882319	15.557056	-0.048308	4.163371
235.728195	5912.922077	15.562061	-0.048326	4.160678
235.566419	5904.967531	15.567066	-0.048291	4.157982
235.454293	5896.906910	15.572071	-0.048265	4.155249
235.484921	5888.899137	15.577075	-0.048265	4.152534
235.652417	5880.843983	15.582080	-0.048291	4.149803
235.525741	5872.876109	15.587085	-0.048263	4.147095
235.541065	5864.854283	15.592090	-0.048261	4.144370
235.606513	5856.905713	15.597095	-0.048268	4.141668
235.459844	5848.886418	15.602099	-0.048236	4.138938
235.242935	5840.912591	15.607104	-0.048190	4.136221
235.474339	5832.854612	15.612109	-0.048228	4.133478
235.399787	5824.897233	15.617114	-0.048209	4.130765
235.145666	5816.866596	15.622119	-0.048157	4.128022
235.082375	5808.895657	15.627123	-0.048140	4.125300
235.095421	5800.903437	15.632128	-0.048138	4.122570
235.061263	5792.917352	15.637133	-0.048126	4.119840
234.961284	5784.941774	15.642138	-0.048103	4.117111
234.936073	5776.906725	15.647143	-0.048093	4.114360
234.817735	5768.907001	15.652147	-0.048066	4.111619
234.684068	5760.833116	15.657152	-0.048036	4.108850
234.866585	5752.842786	15.662157	-0.048065	4.106112
234.997751	5744.867867	15.667162	-0.048085	4.103377
234.743383	5736.893053	15.672167	-0.048032	4.100635
234.842494	5728.937267	15.677171	-0.048046	4.097902
234.628808	5720.903611	15.682176	-0.048001	4.095137
234.653994	5712.886104	15.687181	-0.048001	4.092378
234.701715	5704.882179	15.692186	-0.048005	4.089622
234.721483	5696.908287	15.697191	-0.048003	4.086875
234.560650	5688.938764	15.702195	-0.047968	4.084125
234.532144	5680.969415	15.707200	-0.047958	4.081375
234.467710	5672.980680	15.712205	-0.047941	4.078616
234.436365	5664.984313	15.717210	-0.047930	4.075852
234.364410	5656.891223	15.722215	-0.047912	4.073053
234.341735	5648.902761	15.727219	-0.047903	4.070289
234.352064	5640.915692	15.732224	-0.047900	4.067524
234.245270	5632.903724	15.737229	-0.047875	4.064746
234.214542	5624.948163	15.742234	-0.047864	4.061988
234.218016	5616.913851	15.747239	-0.047860	4.059200
234.324902	5608.982348	15.752243	-0.047875	4.056448
234.138556	5600.929188	15.757248	-0.047835	4.053648
234.246272	5592.895378	15.762253	-0.047850	4.050857
234.161223	5584.950546	15.767258	-0.047829	4.048091
234.139502	5576.906305	15.772263	-0.047820	4.045291
234.054567	5568.981426	15.777267	-0.047799	4.042529
234.032108	5560.931317	15.782272	-0.047790	4.039722
234.027400	5552.966572	15.787277	-0.047784	4.036943
233.991856	5544.927294	15.792282	-0.047773	4.034136
233.844250	5536.793962	15.797287	-0.047740	4.031293
233.997467	5528.873860	15.802291	-0.047764	4.028526
233.829584	5520.867898	15.807296	-0.047727	4.025723
233.755332	5512.907165	15.812301	-0.047708	4.022935
233.709333	5504.898180	15.817306	-0.047695	4.020129
233.503488	5496.944621	15.822311	-0.047652	4.017338
233.547185	5488.930432	15.827315	-0.047655	4.014527
233.511585	5480.899603	15.832320	-0.047643	4.011707
233.665606	5472.869491	15.837325	-0.047667	4.008888
233.627801	5464.914865	15.842330	-0.047655	4.006091
233.366800	5456.911152	15.847335	-0.047601	4.003272
233.401519	5448.924582	15.852339	-0.047603	4.000461
233.412407	5440.965081	15.857344	-0.047600	3.997657
233.308529	5432.920815	15.862349	-0.047575	3.994819
233.453880	5424.890311	15.867354	-0.047597	3.991988
233.225922	5416.847337	15.872359	-0.047550	3.989145
233.252798	5408.945899	15.877363	-0.047550	3.986354
233.217859	5400.898388	15.882368	-0.047538	3.983508
233.055842	5392.930517	15.887373	-0.047503	3.980687
232.972060	5384.960288	15.892378	-0.047483	3.977864
232.936349	5376.938878	15.897383	-0.047471	3.975021
232.875051	5368.959649	15.902387	-0.047455	3.972191
232.793437	5360.901785	15.907392	-0.047434	3.969330
232.928536	5352.948412	15.912397	-0.047455	3.966509
232.910644	5344.963189	15.917402	-0.047446	3.963671
232.854649	5336.996065	15.922407	-0.047431	3.960837
232.763698	5329.008295	15.927411	-0.047409	3.957994
232.848854	5320.982709	15.932416	-0.047420	3.955137
232.855256	5312.920311	15.937421	-0.047416	3.952264
232.761680	5304.934305	15.942426	-0.047394	3.949415
232.540876	5296.965604	15.947431	-0.047348	3.946567
232.618005	5288.965345	15.952435	-0.047357	3.943712
232.482127	5281.006721	15.957440	-0.047327	3.940865
232.314944	5272.980421	15.962445	-0.047290	3.937991
232.394472	5264.998327	15.967450	-0.047300	3.935136
232.166232	5256.953760	15.972455	-0.047253	3.932251
232.279617	5248.961590	15.977459	-0.047269	3.929388
232.382850	5241.003558	15.982464	-0.047283	3.926536
232.376134	5233.006413	15.987469	-0.047277	3.923665
232.396509	5225.008540	15.992474	-0.047276	3.920792
232.243445	5216.997596	15.997479	-0.047242	3.917910
232.016856	5209.005062	16.002483	-0.047195	3.915030
232.062141	5200.986325	16.007488	-0.047198	3.912144
232.119523	5192.961606	16.012493	-0.047204	3.909254
232.052256	5185.003795	16.017498	-0.047187	3.906384
232.013449	5176.976002	16.022503	-0.047174	3.903487
232.208894	5168.997280	16.027507	-0.047206	3.900610
231.987161	5161.047088	16.032512	-0.047160	3.897733
232.018396	5152.948028	16.037517	-0.047160	3.894805
231.869423	5144.995644	16.042522	-0.047128	3.891924
231.667488	5136.980499	16.047527	-0.047085	3.889017
231.554609	5129.022675	16.052531	-0.047059	3.886131
231.910217	5120.972681	16.057536	-0.047120	3.883218
231.751770	5112.980185	16.062541	-0.047086	3.880314
231.720207	5105.046209	16.067546	-0.047075	3.877432
231.671707	5097.010893	16.072551	-0.047061	3.874510
231.615616	5088.764182	16.077555	-0.047045	3.871508
231.469379	5080.845955	16.082560	-0.047013	3.868623
231.483874	5072.888965	16.087565	-0.047011	3.865724
231.658287	5064.938609	16.092570	-0.047038	3.862829
231.279091	5056.939015	16.097575	-0.046963	3.859902
231.513957	5049.022068	16.102579	-0.047001	3.857016
231.502265	5040.979410	16.107584	-0.046994	3.854076
231.409545	5032.988354	16.112589	-0.046972	3.851152
231.371248	5025.002089	16.117594	-0.046960	3.848228
231.333432	5016.968212	16.122599	-0.046948	3.845285
231.216619	5009.026669	16.127603	-0.046921	3.842371
231.104406	5001.005875	16.132608	-0.046895	3.839427
230.913576	4993.073933	16.137613	-0.046855	3.836511
230.888690	4985.080948	16.142618	-0.046845	3.833574
230.844261	4976.997611	16.147623	-0.046832	3.830601
230.893543	4969.019545	16.152627	-0.046836	3.827666
230.988317	4961.022946	16.157632	-0.046849	3.824723
230.896360	4953.045730	16.162637	-0.046827	3.821781
230.999392	4945.070236	16.167642	-0.046841	3.818842
230.893290	4937.069814	16.172647	-0.046816	3.815887
230.806338	4929.099876	16.177651	-0.046795	3.812941
230.517276	4921.037317	16.182656	-0.046736	3.809954
230.814863	4913.059988	16.187661	-0.046786	3.807009
230.750263	4905.073684	16.192666	-0.046769	3.804050
230.340368	4897.132449	16.197671	-0.046688	3.801099
230.322173	4889.113878	16.202675	-0.046680	3.798125
230.398522	4881.127120	16.207680	-0.046689	3.795162
230.318597	4873.028134	16.212685	-0.046669	3.792152
230.279191	4865.074250	16.217690	-0.046657	3.789195
230.375830	4857.046327	16.222695	-0.046670	3.786211
230.350554	4849.104930	16.227699	-0.046660	3.783253
230.148466	4841.095796	16.232704	-0.046617	3.780265
230.141330	4833.113969	16.237709	-0.046611	3.777288
230.214906	4825.103453	16.242714	-0.046620	3.774301
229.931354	4817.060775	16.247719	-0.046562	3.771290
230.239722	4809.072088	16.252723	-0.046614	3.768311
230.072330	4801.082784	16.257728	-0.046578	3.765319
229.952307	4793.122849	16.262733	-0.046551	3.762336
229.977347	4785.094565	16.267738	-0.046551	3.759329
230.017339	4777.135861	16.272743	-0.046553	3.756345
229.922460	4769.117801	16.277747	-0.046530	3.753334
229.964212	4761.060353	16.282752	-0.046533	3.750309
229.819431	4753.108182	16.287757	-0.046501	3.747316
229.801142	4745.064109	16.292762	-0.046493	3.744290
229.626445	4737.125873	16.297767	-0.046455	3.741297
229.848371	4729.133534	16.302771	-0.046492	3.738291
229.919531	4721.102417	16.307776	-0.046500	3.735264
229.663996	4713.131514	16.312781	-0.046447	3.732250
229.596120	4705.115608	16.317786	-0.046430	3.729221
229.609486	4697.121722	16.322791	-0.046427	3.726199
229.724576	4689.151752	16.327795	-0.046444	3.723187
229.512739	4681.181086	16.332800	-0.046399	3.720164
229.597761	4673.208648	16.337805	-0.046410	3.717145
229.570774	4665.202141	16.342810	-0.046400	3.714108
229.274428	4657.087222	16.347815	-0.046340	3.711020
229.180042	4649.123019	16.352819	-0.046317	3.707993
229.318109	4641.107583	16.357824	-0.046338	3.704949
229.155264	4633.166676	16.362829	-0.046303	3.701923
229.024811	4625.199899	16.367834	-0.046273	3.698886
228.936321	4617.190307	16.372839	-0.046252	3.695831
228.997065	4609.223387	16.377843	-0.046258	3.692794
228.717609	4601.193058	16.382848	-0.046201	3.689721
228.815465	4593.199321	16.387853	-0.046214	3.686669
229.040169	4585.184168	16.392858	-0.046251	3.683610
228.947265	4577.208119	16.397863	-0.046229	3.680555
228.914728	4569.275450	16.402867	-0.046218	3.677516
229.011626	4561.233243	16.407872	-0.046231	3.674435
229.057651	4553.212543	16.412877	-0.046235	3.671359
228.774133	4545.242667	16.417882	-0.046177	3.668292
228.576505	4537.216952	16.422887	-0.046135	3.665202
228.786462	4529.245969	16.427891	-0.046169	3.662142
228.816523	4521.235404	16.432896	-0.046170	3.659059
228.580662	4513.279649	16.437901	-0.046121	3.655987
228.654358	4505.242393	16.442906	-0.046129	3.652890
228.512535	4497.230720	16.447911	-0.046098	3.649794
228.447208	4489.265097	16.452915	-0.046081	3.646715
228.468151	4481.262358	16.457920	-0.046080	3.643622
228.293369	4473.266210	16.462925	-0.046042	3.640524
228.332111	4465.297630	16.467930	-0.046045	3.637439
228.291571	4457.271253	16.472935	-0.046032	3.634327
228.402153	4449.249301	16.477939	-0.046048	3.631218
228.099244	4441.265447	16.482944	-0.045986	3.628110
227.816862	4433.270274	16.487949	-0.045929	3.624995
228.187885	4425.299632	16.492954	-0.045993	3.621906
228.008260	4417.295017	16.497959	-0.045954	3.618785
227.946461	4409.324322	16.502963	-0.045938	3.615678
228.008397	4401.308539	16.507968	-0.045944	3.612554
227.979655	4393.286910	16.512973	-0.045934	3.609423
227.849732	4385.356156	16.517978	-0.045905	3.606321
227.766533	4377.324386	16.522983	-0.045884	3.603179
227.884617	4369.374589	16.527987	-0.045901	3.600072
227.707266	4361.393834	16.532992	-0.045863	3.596941
227.733825	4353.358473	16.537997	-0.045863	3.593792
227.708275	4345.352996	16.543002	-0.045853	3.590651
227.465044	4337.362336	16.548007	-0.045803	3.587506
227.534360	4329.356134	16.553011	-0.045811	3.584362
227.524187	4321.411105	16.558016	-0.045804	3.581236
227.702100	4313.388767	16.563021	-0.045832	3.578083
227.678669	4305.399227	16.568026	-0.045823	3.574934
227.475938	4297.409307	16.573031	-0.045780	3.571777
227.553447	4289.405169	16.578035	-0.045790	3.568620
227.394656	4281.428651	16.583040	-0.045755	3.565464
227.128133	4273.445921	16.588045	-0.045701	3.562300
227.275409	4265.434250	16.593050	-0.045723	3.559133
227.311774	4257.448910	16.598055	-0.045725	3.555971
227.210357	4249.367586	16.603059	-0.045701	3.552764
227.118646	4241.335347	16.608064	-0.045679	3.549573
227.103019	4233.369103	16.613069	-0.045671	3.546408
226.888453	4225.429616	16.618074	-0.045626	3.543245
226.630568	4217.419021	16.623079	-0.045573	3.540050
226.789156	4209.431387	16.628083	-0.045597	3.536873
226.873458	4201.425166	16.633088	-0.045608	3.533684
226.829257	4193.411634	16.638093	-0.045595	3.530486
226.854043	4185.448593	16.643098	-0.045595	3.527306
226.834551	4177.403980	16.648103	-0.045586	3.524090
226.849604	4169.489659	16.653107	-0.045584	3.520924
226.747458	4161.511944	16.658112	-0.045560	3.517726
226.634694	4153.483960	16.663117	-0.045534	3.514505
226.689644	4145.473044	16.668122	-0.045539	3.511292
226.520453	4137.466525	16.673127	-0.045503	3.508072
226.740965	4129.459040	16.678131	-0.045539	3.504860
226.768938	4121.521043	16.683136	-0.045539	3.501668
226.526956	4113.525237	16.688141	-0.045489	3.498441
226.535093	4105.573183	16.693146	-0.045485	3.495236
226.355638	4097.542516	16.698151	-0.045447	3.491991
226.367071	4089.532276	16.703155	-0.045444	3.488757
226.095980	4081.589472	16.708160	-0.045389	3.485538
226.112126	4073.609933	16.713165	-0.045387	3.482310
226.491489	4065.584478	16.718170	-0.045452	3.479073
226.252120	4057.642967	16.723175	-0.045403	3.475846
226.149193	4049.588899	16.728179	-0.045379	3.472576
226.193810	4041.573782	16.733184	-0.045382	3.469323
226.031402	4033.590336	16.738189	-0.045347	3.466073
226.066280	4025.595636	16.743194	-0.045348	3.462821
225.875313	4017.620379	16.748199	-0.045308	3.459568
225.917859	4009.635513	16.753203	-0.045310	3.456315
225.709358	4001.669927	16.758208	-0.045267	3.453058
225.634702	3993.622458	16.763213	-0.045248	3.449769
225.515152	3985.661908	16.768218	-0.045221	3.446511
225.303094	3977.664577	16.773223	-0.045176	3.443232
225.623326	3969.646982	16.778227	-0.045231	3.439960
225.629208	3961.688342	16.783232	-0.045227	3.436697
225.297658	3953.668966	16.788237	-0.045160	3.433396
225.504082	3945.637019	16.793242	-0.045193	3.430104
225.332193	3937.645221	16.798247	-0.045156	3.426813
225.537868	3929.655186	16.803251	-0.045190	3.423532
225.403617	3921.710564	16.808256	-0.045160	3.420255
225.498128	3913.691918	16.813261	-0.045172	3.416952
225.732002	3905.721627	16.818266	-0.045211	3.413671
225.337754	3897.703723	16.823271	-0.045133	3.410346
225.350628	3889.730921	16.828275	-0.045130	3.407049
225.323438	3881.722428	16.833280	-0.045120	3.403734
225.254474	3873.762904	16.838285	-0.045102	3.400434
225.007329	3865.820038	16.843290	-0.045051	3.397131
225.023717	3857.771194	16.848295	-0.045049	3.393791
224.968347	3849.692750	16.853299	-0.045034	3.390432
224.833266	3841.738594	16.858304	-0.045004	3.387119
224.872577	3833.742328	16.863309	-0.045006	3.383791
225.160986	3825.782238	16.868314	-0.045055	3.380484
224.901391	3817.811238	16.873319	-0.045001	3.377150
224.913072	3809.834876	16.878323	-0.044999	3.373820
224.872441	3801.811870	16.883328	-0.044986	3.370465
224.625254	3793.836154	16.888333	-0.044935	3.367119
224.487180	3785.876278	16.893338	-0.044904	3.363780
224.342683	3777.887709	16.898343	-0.044873	3.360426
224.450279	3769.880296	16.903347	-0.044888	3.357069
224.416172	3761.887120	16.908352	-0.044876	3.353711
224.305069	3753.826256	16.913357	-0.044850	3.350317
224.504412	3745.856443	16.918362	-0.044883	3.346970
224.198669	3737.881332	16.923367	-0.044821	3.343598
224.197521	3729.895313	16.928371	-0.044816	3.340230
224.250951	3721.929593	16.933376	-0.044820	3.336869
224.120081	3713.909720	16.938381	-0.044791	3.333474
224.202647	3705.913318	16.943386	-0.044801	3.330094
224.055996	3697.948801	16.948391	-0.044769	3.326716
224.006621	3689.946351	16.953395	-0.044755	3.323322
223.966756	3681.981414	16.958400	-0.044743	3.319940
223.970037	3674.017130	16.963405	-0.044738	3.316557
223.921054	3666.000291	16.968410	-0.044724	3.313147
223.828161	3657.961178	16.973415	-0.044702	3.309721
223.686895	3649.999912	16.978419	-0.044671	3.306324
223.797544	3641.981288	16.983424	-0.044686	3.302907
223.843412	3633.990582	16.988429	-0.044690	3.299497
223.935974	3626.057231	16.993434	-0.044702	3.296110
224.053697	3618.023263	16.998439	-0.044719	3.292677
223.971312	3610.036008	17.003443	-0.044699	3.289253
223.748035	3602.100371	17.008448	-0.044652	3.285842
223.477279	3594.106853	17.013453	-0.044597	3.282400
223.622347	3586.097303	17.018458	-0.044619	3.278964
223.390546	3578.141859	17.023463	-0.044570	3.275534
223.567186	3570.093979	17.028467	-0.044598	3.272075
223.441859	3562.107359	17.033472	-0.044570	3.268628
223.367112	3554.093517	17.038477	-0.044551	3.265167
223.209884	3546.164380	17.043482	-0.044517	3.261736
223.023315	3538.167696	17.048487	-0.044477	3.258271
223.000551	3530.174663	17.053491	-0.044468	3.254810
223.096432	3522.161225	17.058496	-0.044481	3.251342
223.125474	3514.157423	17.063501	-0.044481	3.247871
223.162597	3506.165012	17.068506	-0.044483	3.244402
223.063536	3498.218868	17.073511	-0.044460	3.240944
222.924662	3490.255553	17.078515	-0.044429	3.237473
222.870257	3482.230681	17.083520	-0.044414	3.233975
222.838715	3474.140845	17.088525	-0.044403	3.230445
222.739140	3466.192005	17.093530	-0.044379	3.226971
222.668660	3458.209076	17.098535	-0.044361	3.223479
222.657699	3450.242091	17.103539	-0.044354	3.219992
222.512074	3442.306368	17.108544	-0.044322	3.216510
222.491017	3434.252307	17.113549	-0.044313	3.212978
222.484423	3426.272568	17.118554	-0.044307	3.209475
222.430741	3418.288249	17.123559	-0.044292	3.205964
222.353152	3410.322771	17.128563	-0.044273	3.202456
222.363454	3402.343550	17.133568	-0.044269	3.198942
222.422410	3394.340866	17.138573	-0.044275	3.195416
222.331987	3386.337191	17.143578	-0.044254	3.191880
222.166266	3378.372220	17.148583	-0.044218	3.188353
222.158705	3370.354460	17.153587	-0.044211	3.184806
222.224511	3362.400604	17.158592	-0.044219	3.181286
222.037937	3354.427691	17.163597	-0.044179	3.177743
222.350377	3346.383387	17.168602	-0.044232	3.174186
222.242275	3338.385707	17.173607	-0.044207	3.170628
222.280985	3330.411629	17.178611	-0.044209	3.167082
222.253828	3322.453543	17.183616	-0.044199	3.163537
222.038409	3314.488372	17.188621	-0.044154	3.159976
222.129927	3306.516424	17.193626	-0.044166	3.156421
221.963757	3298.484955	17.198631	-0.044130	3.152825
221.833498	3290.470388	17.203635	-0.044101	3.149234
221.972895	3282.479060	17.208640	-0.044122	3.145661
221.878702	3274.489716	17.213645	-0.044099	3.142074
221.775383	3266.525036	17.218650	-0.044075	3.138494
221.683112	3258.570494	17.223655	-0.044053	3.134915
221.691381	3250.558308	17.228659	-0.044050	3.131311
221.621680	3242.607378	17.233664	-0.044032	3.127726
221.586629	3234.561852	17.238669	-0.044020	3.124096
221.873219	3226.605061	17.243674	-0.044068	3.120516
221.674789	3218.628830	17.248679	-0.044027	3.116902
221.632586	3210.665704	17.253683	-0.044014	3.113296
221.449040	3202.658437	17.258688	-0.043975	3.109660
221.404582	3194.650857	17.263693	-0.043961	3.106026
221.460425	3186.684540	17.268698	-0.043967	3.102411
221.372314	3178.686340	17.273703	-0.043945	3.098770
221.370866	3170.725887	17.278707	-0.043940	3.095146
221.133335	3162.753350	17.283712	-0.043891	3.091502
221.082791	3154.733175	17.288717	-0.043876	3.087840
221.123321	3146.748167	17.293722	-0.043879	3.084194
221.127746	3138.778968	17.298727	-0.043875	3.080550
221.065396	3130.793269	17.303731	-0.043858	3.076890
221.100266	3122.771150	17.308736	-0.043860	3.073214
220.698770	3114.735772	17.313741	-0.043780	3.069507
220.843032	3106.761875	17.318746	-0.043802	3.065849
220.901442	3098.780433	17.323751	-0.043808	3.062179
221.052192	3090.801781	17.328755	-0.043831	3.058511
220.690495	3082.900105	17.333760	-0.043759	3.054850
220.876046	3074.851138	17.338765	-0.043788	3.051142
220.719584	3066.897713	17.343770	-0.043754	3.047457
220.375551	3058.934254	17.348775	-0.043685	3.043754
220.426121	3050.939857	17.353779	-0.043689	3.040052
220.447722	3042.973642	17.358784	-0.043688	3.036356
220.417083	3034.917774	17.363789	-0.043678	3.032612
220.424841	3026.954403	17.368794	-0.043674	3.028908
220.331991	3018.977757	17.373799	-0.043652	3.025188
220.193732	3011.011027	17.378803	-0.043621	3.021467
220.430363	3003.016319	17.383808	-0.043660	3.017746
220.308989	2995.030813	17.388813	-0.043633	3.014007
220.353032	2987.029920	17.393818	-0.043636	3.010264
220.224866	2979.068381	17.398823	-0.043607	3.006527
220.236761	2971.090751	17.403827	-0.043604	3.002784
220.176026	2963.138032	17.408832	-0.043588	2.999045
219.945969	2955.163419	17.413837	-0.043540	2.995282
220.137949	2947.103901	17.418842	-0.043571	2.991496
219.872985	2939.140024	17.423847	-0.043517	2.987727
219.811510	2931.151488	17.428851	-0.043500	2.983952
219.737875	2923.201446	17.433856	-0.043481	2.980189
219.626961	2915.221301	17.438861	-0.043456	2.976406
219.747037	2907.211532	17.443866	-0.043473	2.972616
219.638651	2899.212714	17.448871	-0.043448	2.968814
219.514850	2891.246863	17.453875	-0.043420	2.965022
219.494348	2883.310985	17.458880	-0.043411	2.961245
219.237665	2875.316367	17.463885	-0.043358	2.957423
219.322807	2867.309742	17.468890	-0.043369	2.953608
219.260463	2859.330005	17.473895	-0.043353	2.949794
219.350737	2851.331712	17.478899	-0.043364	2.945973
219.463637	2843.366050	17.483904	-0.043381	2.942164
219.313616	2835.368935	17.488909	-0.043348	2.938321
219.504428	2827.373864	17.493914	-0.043378	2.934493
219.179349	2819.399288	17.498919	-0.043313	2.930642
219.168165	2811.421179	17.503923	-0.043306	2.926800
219.217535	2803.455341	17.508928	-0.043310	2.922963
218.921885	2795.500902	17.513933	-0.043250	2.919108
218.992054	2787.513096	17.518938	-0.043258	2.915251
218.806305	2779.454377	17.523943	-0.043218	2.911341
218.775040	2771.464888	17.528947	-0.043207	2.907468
218.950644	2763.473519	17.533952	-0.043235	2.903599
218.601572	2755.550068	17.538957	-0.043165	2.899730
218.612563	2747.591090	17.543962	-0.043162	2.895859
218.662406	2739.572485	17.548967	-0.043167	2.891954
218.442485	2731.598496	17.553971	-0.043121	2.888052
218.601729	2723.625762	17.558976	-0.043145	2.884166
218.587832	2715.651747	17.563981	-0.043138	2.880264
218.686929	2707.692480	17.568986	-0.043151	2.876371
218.551252	2699.698973	17.573991	-0.043121	2.872443
218.406544	2691.695890	17.578995	-0.043089	2.868504
218.236364	2683.732110	17.584000	-0.043052	2.864577
218.305461	2675.758761	17.589005	-0.043060	2.860654
218.485979	2667.778065	17.594010	-0.043089	2.856727
218.466015	2659.786023	17.599015	-0.043080	2.852779
218.159753	2651.817238	17.604019	-0.043018	2.848821
218.255125	2643.844444	17.609024	-0.043031	2.844877
218.029913	2635.900150	17.614029	-0.042984	2.840924
218.378415	2627.904352	17.619034	-0.043044	2.836973
218.221992	2619.909860	17.624039	-0.043010	2.832988
218.072478	2611.902737	17.629043	-0.042977	2.828991
218.074949	2603.922802	17.634048	-0.042972	2.825012
217.932062	2595.960747	17.639053	-0.042941	2.821027
218.029237	2587.989369	17.644058	-0.042954	2.817045
217.921456	2580.012248	17.649063	-0.042929	2.813043
217.761388	2572.018963	17.654067	-0.042894	2.809025
217.681881	2564.062704	17.659072	-0.042874	2.805024
217.725266	2556.085056	17.664077	-0.042877	2.801013
217.593673	2548.129741	17.669082	-0.042848	2.796998
217.434065	2540.147112	17.674087	-0.042813	2.792961
217.517235	2532.120173	17.679091	-0.042824	2.788911
217.373529	2524.174976	17.684096	-0.042792	2.784883
217.418067	2516.189899	17.689101	-0.042795	2.780839
217.470198	2508.228436	17.694106	-0.042800	2.776802
217.438337	2500.237369	17.699111	-0.042789	2.772740
217.144178	2492.268466	17.704115	-0.042729	2.768667
217.154998	2484.283694	17.709120	-0.042726	2.764598
217.046347	2476.338130	17.714125	-0.042701	2.760536
217.108007	2468.378816	17.719130	-0.042708	2.756471
217.067573	2460.329266	17.724135	-0.042695	2.752348
216.913965	2452.316700	17.729139	-0.042662	2.748231
216.921503	2444.348842	17.734144	-0.042658	2.744140
216.752128	2436.409534	17.739149	-0.042622	2.740047
216.847612	2428.442327	17.744154	-0.042634	2.735950
216.902896	2420.440963	17.749159	-0.042640	2.731826
216.786217	2412.468459	17.754163	-0.042613	2.727701
216.815498	2404.516032	17.759168	-0.042613	2.723588
216.627675	2396.555722	17.764173	-0.042574	2.719452
216.776323	2388.601111	17.769178	-0.042596	2.715334
216.617894	2380.596169	17.774183	-0.042562	2.711164
216.583805	2372.612707	17.779187	-0.042550	2.707006
216.500564	2364.667771	17.784192	-0.042530	2.702859
216.395794	2356.698823	17.789197	-0.042505	2.698692
216.457406	2348.730563	17.794202	-0.042512	2.694529
216.227039	2340.747243	17.799207	-0.042464	2.690333
216.196904	2332.749351	17.804211	-0.042453	2.686136
216.297084	2324.795119	17.809216	-0.042467	2.681964
216.250114	2316.824197	17.814221	-0.042453	2.677766
216.121071	2308.873979	17.819226	-0.042424	2.673568
215.790303	2300.878101	17.824231	-0.042358	2.669326
215.817164	2292.883448	17.829235	-0.042358	2.665101
216.102622	2284.905859	17.834240	-0.042406	2.660895
215.869230	2276.955845	17.839245	-0.042358	2.656664
215.919493	2268.966907	17.844250	-0.042362	2.652423
215.870514	2260.986159	17.849255	-0.042348	2.648174
215.708743	2253.007502	17.854259	-0.042313	2.643911
215.461797	2245.105157	17.859264	-0.042262	2.639677
215.617552	2237.111222	17.864269	-0.042286	2.635413
215.726853	2229.095954	17.869274	-0.042301	2.631128
215.578072	2221.126120	17.874279	-0.042269	2.626843
215.489735	2213.185124	17.879283	-0.042247	2.622571
215.702480	2205.196060	17.884288	-0.042282	2.618286
215.512317	2197.245617	17.889293	-0.042241	2.613987
215.462876	2189.262277	17.894298	-0.042227	2.609674
215.441953	2181.304475	17.899303	-0.042218	2.605369
215.225321	2173.364070	17.904307	-0.042173	2.601053
215.244121	2165.404707	17.909312	-0.042172	2.596735
215.098119	2157.306995	17.914317	-0.042139	2.592324
215.009539	2149.263226	17.919322	-0.042118	2.587938
215.053936	2141.311124	17.924327	-0.042121	2.583605
215.041194	2133.388646	17.929331	-0.042114	2.579276
215.105736	2125.451793	17.934336	-0.042121	2.574937
214.831950	2117.485815	17.939341	-0.042065	2.570552
214.930007	2109.524456	17.944346	-0.042078	2.566187
214.850341	2101.598467	17.949351	-0.042058	2.561822
214.816054	2093.619139	17.954355	-0.042047	2.557424
214.871915	2085.647499	17.959360	-0.042052	2.553028
214.777575	2077.662630	17.964365	-0.042030	2.548607
214.720015	2069.708394	17.969370	-0.042014	2.544198
214.885381	2061.737908	17.974375	-0.042040	2.539788
214.732103	2053.795409	17.979379	-0.042007	2.535363
214.588814	2045.843456	17.984384	-0.041975	2.530926
214.571135	2037.857304	17.989389	-0.041967	2.526471
214.434252	2029.916423	17.994394	-0.041936	2.522024
214.458656	2021.957508	17.999399	-0.041936	2.517572
214.166970	2013.985944	18.004403	-0.041876	2.513081
214.334138	2005.979480	18.009408	-0.041903	2.508597
214.129601	1998.011563	18.014413	-0.041860	2.504098
214.342525	1990.053732	18.019418	-0.041894	2.499628
214.065273	1982.127229	18.024423	-0.041838	2.495132
213.875809	1974.149231	18.029427	-0.041797	2.490605
214.073419	1966.158239	18.034432	-0.041829	2.486090
213.774264	1958.224696	18.039437	-0.041769	2.481564
214.033245	1950.244210	18.044442	-0.041812	2.477043
213.801343	1942.302630	18.049447	-0.041764	2.472500
213.804387	1934.301441	18.054451	-0.041759	2.467933
213.820757	1926.355031	18.059456	-0.041757	2.463389
213.600230	1918.404715	18.064461	-0.041711	2.458816
213.602558	1910.443118	18.069466	-0.041707	2.454246
213.699633	1902.463038	18.074471	-0.041720	2.449663
213.367222	1894.524739	18.079475	-0.041653	2.445063
213.610654	1886.555810	18.084480	-0.041693	2.440481
213.495792	1878.610873	18.089485	-0.041667	2.435877
213.377571	1870.599930	18.094490	-0.041640	2.431225
213.326342	1862.618362	18.099495	-0.041625	2.426587
213.125114	1854.670588	18.104499	-0.041583	2.421948
213.136740	1846.739652	18.109504	-0.041580	2.417326
213.048799	1838.760441	18.114509	-0.041559	2.412659
213.181834	1830.775610	18.119514	-0.041579	2.407997
213.209603	1822.828669	18.124519	-0.041579	2.403341
212.981457	1814.899089	18.129523	-0.041531	2.398665
213.265320	1806.935580	18.134528	-0.041579	2.394000
212.953614	1798.980267	18.139533	-0.041516	2.389285
212.852106	1791.029607	18.144538	-0.041492	2.384579
212.885577	1783.077921	18.149543	-0.041494	2.379874
212.774494	1775.123478	18.154547	-0.041468	2.375146
212.942763	1767.139509	18.159552	-0.041494	2.370414
212.673894	1759.198270	18.164557	-0.041439	2.365663
212.773909	1751.246151	18.169562	-0.041453	2.360925
212.749333	1743.306660	18.174567	-0.041444	2.356176
212.463001	1735.339979	18.179571	-0.041385	2.351379
212.475739	1727.375989	18.184576	-0.041383	2.346598
212.358122	1719.409599	18.189581	-0.041356	2.341796
212.297979	1711.482076	18.194586	-0.041340	2.337011
212.094152	1703.528403	18.199591	-0.041297	2.332189
212.342539	1695.528439	18.204595	-0.041338	2.327367
212.235014	1687.620401	18.209600	-0.041313	2.322561
211.985269	1679.679466	18.214605	-0.041262	2.317713
212.092189	1671.715744	18.219610	-0.041276	2.312870
212.022390	1663.740196	18.224615	-0.041259	2.307996
211.792598	1655.802196	18.229619	-0.041211	2.303121
211.898851	1647.856621	18.234624	-0.041226	2.298258
211.914620	1639.887425	18.239629	-0.041224	2.293364
211.768993	1631.944779	18.244634	-0.041191	2.288462
211.690545	1624.007699	18.249639	-0.041172	2.283558
211.678594	1616.046751	18.254643	-0.041165	2.278634
211.649525	1608.096061	18.259648	-0.041154	2.273705
211.341339	1600.108114	18.264653	-0.041092	2.268718
211.567666	1592.123187	18.269658	-0.041129	2.263768
211.413965	1584.215576	18.274663	-0.041096	2.258823
211.275029	1576.258717	18.279667	-0.041065	2.253837
211.328824	1568.293706	18.284672	-0.041070	2.248851
211.179130	1560.367725	18.289677	-0.041037	2.243861
211.179221	1552.439046	18.294682	-0.041032	2.238872
211.153533	1544.495536	18.299687	-0.041022	2.233860
211.186816	1536.511280	18.304691	-0.041024	2.228816
211.356376	1528.558933	18.309696	-0.041050	2.223793
211.177964	1520.645524	18.314701	-0.041012	2.218752
211.007412	1512.717010	18.319706	-0.040975	2.213691
211.125188	1504.735345	18.324711	-0.040992	2.208610
210.925808	1496.821046	18.329715	-0.040950	2.203532
210.970550	1488.886276	18.334720	-0.040954	2.198451
210.883997	1480.948066	18.339725	-0.040932	2.193344
210.842764	1472.969908	18.344730	-0.040920	2.188203
210.637586	1465.042685	18.349735	-0.040877	2.183069
210.723396	1457.084989	18.354739	-0.040888	2.177929
210.770695	1449.138006	18.359744	-0.040891	2.172781
210.590933	1441.202540	18.364749	-0.040853	2.167606
210.543673	1433.276824	18.369754	-0.040839	2.162438
210.693783	1425.320182	18.374759	-0.040862	2.157256
210.525075	1417.392601	18.379763	-0.040826	2.152051
210.505740	1409.445114	18.384768	-0.040817	2.146834
210.278228	1401.529229	18.389773	-0.040770	2.141605
210.320821	1393.587217	18.394778	-0.040773	2.136372
210.482405	1385.626767	18.399783	-0.040798	2.131125
210.306835	1377.687465	18.404787	-0.040761	2.125846
210.184707	1369.789861	18.409792	-0.040733	2.120588
210.211415	1361.846675	18.414797	-0.040733	2.115301
210.027872	1353.853503	18.419802	-0.040694	2.109946
209.980344	1345.922322	18.424807	-0.040680	2.104632
209.703972	1338.017607	18.429811	-0.040624	2.099301
209.621175	1330.106944	18.434816	-0.040603	2.093971
209.734783	1322.114679	18.439821	-0.040619	2.088591
209.645557	1314.188293	18.444826	-0.040598	2.083222
209.493908	1306.300671	18.449831	-0.040565	2.077860
209.652048	1298.328719	18.454835	-0.040589	2.072456
209.572431	1290.407540	18.459840	-0.040569	2.067050
209.415493	1282.481691	18.464845	-0.040535	2.061618
209.400042	1274.566361	18.469850	-0.040527	2.056194
209.451858	1266.612578	18.474855	-0.040532	2.050735
209.277138	1258.692323	18.479859	-0.040495	2.045263
209.322372	1250.770318	18.484864	-0.040498	2.039796
209.193381	1242.861352	18.489869	-0.040469	2.034306
208.933404	1234.928222	18.494874	-0.040416	2.028771
209.037349	1226.972426	18.499879	-0.040430	2.023243
209.335943	1219.002824	18.504883	-0.040481	2.017709
209.273952	1211.113263	18.509888	-0.040464	2.012180
209.015653	1203.198537	18.514893	-0.040411	2.006597
208.753862	1195.312070	18.519898	-0.040358	2.001017
208.711977	1187.400342	18.524903	-0.040345	1.995428
208.763073	1179.442801	18.529907	-0.040349	1.989800
208.761576	1171.515093	18.534912	-0.040344	1.984171
208.582691	1163.617238	18.539917	-0.040306	1.978529
208.500932	1155.712908	18.544922	-0.040286	1.972877
208.419650	1147.780911	18.549927	-0.040266	1.967189
208.328170	1139.858442	18.554931	-0.040244	1.961489
208.295854	1131.963384	18.559936	-0.040233	1.955800
208.268917	1123.976339	18.564941	-0.040223	1.950027
208.273303	1116.044374	18.569946	-0.040219	1.944281
208.059883	1108.178009	18.574951	-0.040174	1.938542
207.900746	1100.247995	18.579955	-0.040139	1.932745
208.060189	1092.304084	18.584960	-0.040164	1.926956
207.996741	1084.393074	18.589965	-0.040147	1.921149
207.909574	1076.503230	18.594970	-0.040126	1.915337
207.857249	1068.587519	18.599975	-0.040111	1.909492
207.852503	1060.656408	18.604979	-0.040106	1.903623
207.855195	1052.770644	18.609984	-0.040101	1.897771
207.795857	1044.852648	18.614989	-0.040085	1.891869
207.458451	1036.972029	18.619994	-0.040017	1.885945
207.633908	1029.048940	18.624999	-0.040045	1.880029
207.469931	1021.165440	18.630003	-0.040010	1.874086
207.513925	1013.227351	18.635008	-0.040013	1.868106
207.293343	1005.333613	18.640013	-0.039967	1.862110
207.160191	997.445913	18.645018	-0.039937	1.856109
207.414892	989.490798	18.650023	-0.039980	1.850082
207.216034	981.602968	18.655027	-0.039938	1.844035
207.112935	973.740270	18.660032	-0.039914	1.837997
206.919703	965.850833	18.665037	-0.039873	1.831909
206.770090	957.950331	18.670042	-0.039840	1.825797
206.826896	950.041731	18.675047	-0.039846	1.819683
206.667470	942.164304	18.680051	-0.039811	1.813546
206.894738	934.221476	18.685056	-0.039848	1.807384
206.854841	926.325503	18.690061	-0.039836	1.801206
206.569298	918.477396	18.695066	-0.039778	1.795013
206.688593	910.503531	18.700071	-0.039795	1.788750
206.520681	902.625516	18.705075	-0.039759	1.782505
206.328838	894.776974	18.710080	-0.039718	1.776259
206.296042	886.865604	18.715085	-0.039707	1.769960
206.196075	878.991483	18.720090	-0.039684	1.763660
206.297215	871.103653	18.725095	-0.039698	1.757352
206.176163	863.216727	18.730099	-0.039670	1.750994
206.123682	855.338132	18.735104	-0.039656	1.744628
206.022159	847.463279	18.740109	-0.039632	1.738235
206.021081	839.580417	18.745114	-0.039627	1.731825
206.113487	831.669245	18.750119	-0.039639	1.725380
205.884669	823.838375	18.755123	-0.039591	1.718936
205.890804	815.953254	18.760128	-0.039588	1.712452
205.775250	808.056146	18.765133	-0.039561	1.705919
205.678842	800.190651	18.770138	-0.039538	1.699389
205.559949	792.341747	18.775143	-0.039511	1.692844
205.469014	784.447002	18.780147	-0.039489	1.686240
205.469558	776.587315	18.785152	-0.039485	1.679651
205.339517	768.742461	18.790157	-0.039456	1.673031
205.324364	760.850383	18.795162	-0.039448	1.666361
205.276553	753.000192	18.800167	-0.039434	1.659695
205.183150	745.125319	18.805171	-0.039412	1.652974
205.353314	737.228672	18.810176	-0.039438	1.646244
205.376400	729.377018	18.815181	-0.039438	1.639504
205.142937	721.533318	18.820186	-0.039390	1.632708
204.983137	713.654368	18.825191	-0.039355	1.625863
204.846688	705.810153	18.830195	-0.039325	1.619023
204.830789	697.962897	18.835200	-0.039317	1.612168
204.698928	690.102746	18.840205	-0.039287	1.605256
204.928660	682.230629	18.845210	-0.039325	1.598354
204.664114	674.423975	18.850215	-0.039271	1.591411
204.598083	666.565997	18.855219	-0.039254	1.584419
204.544748	658.736810	18.860224	-0.039239	1.577424
204.669020	650.852855	18.865229	-0.039257	1.570375
204.456735	643.051552	18.870234	-0.039213	1.563319
204.505589	635.218064	18.875239	-0.039217	1.556240
204.473443	627.353163	18.880243	-0.039206	1.549089
204.344020	619.541161	18.885248	-0.039177	1.541938
204.277673	611.713617	18.890253	-0.039160	1.534749
204.231736	603.866524	18.895258	-0.039146	1.527511
204.069795	596.075296	18.900263	-0.039111	1.520273
203.862398	588.276951	18.905267	-0.039068	1.512987
203.922822	580.431159	18.910272	-0.039074	1.505662
203.845165	572.623720	18.915277	-0.039055	1.498316
203.628326	564.820908	18.920282	-0.039010	1.490916
203.604392	557.004903	18.925287	-0.039000	1.483497
203.560093	549.191745	18.930291	-0.038987	1.476040
203.521557	541.337141	18.935296	-0.038975	1.468507
203.219699	533.562154	18.940301	-0.038914	1.460970
203.318617	525.736570	18.945306	-0.038928	1.453408
203.364819	517.915853	18.950311	-0.038931	1.445803
203.194666	510.154271	18.955315	-0.038895	1.438181
203.132672	502.362599	18.960320	-0.038878	1.430506
203.168650	494.555282	18.965325	-0.038880	1.422790
202.930797	486.805691	18.970330	-0.038831	1.415045
202.847015	479.019030	18.975335	-0.038811	1.407245
202.983590	471.209121	18.980339	-0.038831	1.399416
203.038039	463.424070	18.985344	-0.038837	1.391553
202.796646	455.671502	18.990349	-0.038787	1.383629
202.720396	447.899849	18.995354	-0.038768	1.375668
202.610218	440.143548	19.000359	-0.038742	1.367670
202.336078	432.409720	19.005363	-0.038687	1.359620
202.442634	424.635970	19.010368	-0.038702	1.351547
202.431613	416.865751	19.015373	-0.038695	1.343409
202.296097	409.129555	19.020378	-0.038665	1.335234
202.041018	401.410145	19.025383	-0.038612	1.327006
201.912068	393.684050	19.030387	-0.038583	1.318742
201.966193	385.845224	19.035392	-0.038589	1.310337
201.887065	378.064934	19.040397	-0.038569	1.301918
201.887125	370.336127	19.045402	-0.038564	1.293514
202.041025	362.587904	19.050407	-0.038588	1.285062
201.930381	354.900882	19.055411	-0.038563	1.276573
201.765765	347.207738	19.060416	-0.038527	1.268010
201.553445	339.532334	19.065421	-0.038483	1.259400
201.401962	331.844203	19.070426	-0.038450	1.250727
201.214660	324.176619	19.075431	-0.038410	1.242010
201.283439	316.455166	19.080435	-0.038418	1.233220
201.329783	308.743638	19.085440	-0.038422	1.224373
200.921003	301.123858	19.090445	-0.038341	1.215479
200.817815	293.440132	19.095450	-0.038317	1.206505
201.008521	285.748721	19.100455	-0.038348	1.197514
200.661133	278.122557	19.105459	-0.038278	1.188423
200.557369	270.475895	19.110464	-0.038254	1.179288
200.651960	262.797597	19.115469	-0.038267	1.170083
200.524810	255.174652	19.120474	-0.038239	1.160827
200.309296	247.558495	19.125479	-0.038194	1.151486
200.146445	239.910905	19.130483	-0.038159	1.142041
200.352638	232.255845	19.135488	-0.038192	1.132587
200.172742	224.661465	19.140493	-0.038154	1.123046
199.932957	217.097188	19.145498	-0.038105	1.113449
200.106391	209.460146	19.150503	-0.038132	1.103765
199.863860	201.905659	19.155507	-0.038083	1.094011
199.534204	194.370701	19.160512	-0.038016	1.084174
199.484085	186.809009	19.165517	-0.038002	1.074275
199.234270	179.258755	19.170522	-0.037951	1.064253
199.117134	171.727662	19.175527	-0.037925	1.054193
198.972778	164.181591	19.180531	-0.037893	1.044008
199.023785	156.646049	19.185536	-0.037898	1.033784
199.065079	149.112552	19.190541	-0.037901	1.023459
198.793863	141.651008	19.195546	-0.037846	1.013053
198.873659	134.131462	19.200551	-0.037856	1.002542
198.665441	126.668656	19.205555	-0.037813	0.991930
198.590910	119.187979	19.210560	-0.037794	0.981211
198.590210	111.725157	19.215565	-0.037789	0.970418
198.288844	104.329777	19.220570	-0.037729	0.959526
198.185139	96.920972	19.225575	-0.037705	0.948540
197.822437	89.556988	19.230579	-0.037632	0.937424
197.862948	82.146139	19.235584	-0.037635	0.926211
197.665242	74.801223	19.240589	-0.037594	0.914898
197.282367	67.478891	19.245594	-0.037518	0.903427
197.105602	60.389748	19.250599	-0.037481	0.892235