Thu Mar 11 19:32:17 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.556814	0.170287	0.000000	0.000021	0.724554

0.773872	0.020159	0.005005	-0.000020	0.724336
0.730079	-0.006016	0.010010	-0.000012	0.724270
0.404080	0.047669	0.015014	0.000049	0.724262
0.565744	0.022226	0.020019	0.000018	0.724269
0.661193	0.004108	0.025024	0.000000	0.724267
0.493228	0.033564	0.030029	0.000031	0.724266
0.747513	-0.010322	0.035034	-0.000016	0.724270
0.569616	0.015401	0.040038	0.000017	0.724258
0.676089	0.000542	0.045043	-0.000003	0.724267
0.675888	0.001046	0.050048	-0.000004	0.724268
0.592972	0.012929	0.055053	0.000012	0.724263
0.736862	-0.007914	0.060058	-0.000015	0.724273
0.595182	0.011760	0.065062	0.000011	0.724262
0.453822	0.039150	0.070067	0.000037	0.724267
0.475341	0.034552	0.075072	0.000033	0.724266
0.495307	-0.086738	0.080077	0.000029	0.724036
0.593973	-0.143481	0.085082	0.000010	0.723959
0.505395	-0.132820	0.090086	0.000026	0.723950
0.633087	-0.151579	0.095091	0.000002	0.723958
0.416219	-0.114492	0.100096	0.000043	0.723955
0.333807	-0.103534	0.105101	0.000058	0.723948
0.648186	-0.157244	0.110106	-0.000001	0.723953
0.349248	-0.268742	0.115110	0.000055	0.723631
0.314073	-0.261891	0.120115	0.000061	0.723633
0.612446	-0.312236	0.125120	0.000005	0.723638
0.595981	-0.313336	0.130125	0.000008	0.723631
0.728280	-0.329931	0.135130	-0.000017	0.723645
0.597619	-0.455156	0.140134	0.000007	0.723354
0.645986	-0.467679	0.145139	-0.000002	0.723347
0.592520	-0.456696	0.150144	0.000008	0.723350
0.555333	-0.455101	0.155149	0.000015	0.723341
0.692367	-0.611013	0.160154	-0.000011	0.723083
0.490437	-0.613946	0.165158	0.000026	0.723007
0.546525	-0.621157	0.170163	0.000016	0.723013
0.697081	-0.670017	0.175168	-0.000013	0.722970
0.742167	-0.818997	0.180173	-0.000021	0.722694
0.370170	-0.749510	0.185178	0.000048	0.722701
0.091901	-0.704308	0.190182	0.000099	0.722693
0.399068	-0.867415	0.195187	0.000042	0.722481
0.197834	-0.884711	0.200192	0.000079	0.722377
0.125811	-0.873884	0.205197	0.000093	0.722373
0.429162	-0.988172	0.210202	0.000036	0.722255
0.287778	-1.052947	0.215206	0.000062	0.722079
0.208469	-1.037842	0.220211	0.000077	0.722081
0.358548	-1.135344	0.225216	0.000049	0.721943
0.353732	-1.235559	0.230221	0.000049	0.721745
0.402529	-1.239809	0.235226	0.000040	0.721754
0.385874	-1.348573	0.240230	0.000043	0.721535
0.339310	-1.387542	0.245235	0.000051	0.721442
0.373331	-1.408737	0.250240	0.000045	0.721413
0.123083	-1.512879	0.255245	0.000091	0.721121
0.341042	-1.546980	0.260250	0.000051	0.721130
0.114709	-1.579702	0.265254	0.000093	0.720987
-0.043173	-1.603493	0.270259	0.000122	0.720886
0.031488	-1.633065	0.275264	0.000108	0.720854
0.097480	-1.804548	0.280269	0.000095	0.720540
0.283429	-1.833390	0.285274	0.000060	0.720549
0.039443	-1.917933	0.290278	0.000106	0.720297
0.316122	-2.001503	0.295283	0.000054	0.720230
0.394977	-2.107266	0.300288	0.000039	0.720050
0.069797	-2.125086	0.305293	0.000100	0.719901
-0.179273	-2.141827	0.310298	0.000146	0.719781
0.036491	-2.269419	0.315302	0.000105	0.719606
-0.042201	-2.307014	0.320307	0.000120	0.719505
-0.340759	-2.368903	0.325312	0.000175	0.719278
-2.601154	-1.971097	0.330317	0.000596	0.719269
-2.675075	-2.090794	0.335322	0.000609	0.719008
-3.551393	-1.956889	0.340326	0.000772	0.718964
-3.823523	-1.906614	0.345331	0.000823	0.718968
-3.210899	-2.099956	0.350336	0.000708	0.718802
-4.391425	-1.970632	0.355341	0.000928	0.718643
-4.253529	-1.990536	0.360346	0.000902	0.718653
-4.544698	-1.944265	0.365350	0.000956	0.718642
-4.670405	-2.045761	0.370355	0.000979	0.718398
-5.258575	-1.960147	0.375360	0.001088	0.718361
-5.704976	-1.882943	0.380365	0.001171	0.718356
-5.377053	-1.937368	0.385370	0.001110	0.718365
-5.469410	-2.021872	0.390374	0.001127	0.718166
-6.381442	-1.932146	0.395379	0.001297	0.718023
-6.254747	-1.954367	0.400384	0.001273	0.718024
-6.349540	-1.939944	0.405389	0.001290	0.718019
-6.263225	-1.952208	0.410394	0.001274	0.718026
-6.821432	-1.993342	0.415398	0.001378	0.717748
-7.456660	-1.899600	0.420403	0.001496	0.717711
-7.110376	-1.962317	0.425408	0.001431	0.717709
-7.255329	-1.939432	0.430413	0.001458	0.717704
-7.330524	-1.920837	0.435418	0.001472	0.717714
-7.420915	-1.991461	0.440422	0.001488	0.717543
-8.425790	-1.891637	0.445427	0.001675	0.717387
-8.180911	-1.934437	0.450432	0.001629	0.717389
-8.151847	-1.943810	0.455437	0.001624	0.717381
-8.162958	-1.938961	0.460442	0.001626	0.717387
-8.548259	-1.874526	0.465446	0.001697	0.717379
-8.470431	-1.956404	0.470451	0.001682	0.717245
-9.131582	-1.917846	0.475456	0.001805	0.717089
-9.088328	-1.930020	0.480461	0.001797	0.717081
-9.093701	-1.924380	0.485466	0.001798	0.717090
-9.303721	-1.890335	0.490470	0.001837	0.717084
-9.225126	-1.904031	0.495475	0.001822	0.717085
-9.349504	-1.902640	0.500480	0.001845	0.717044
-10.191249	-1.899724	0.505485	0.002001	0.716754
-9.842320	-1.957591	0.510490	0.001936	0.716763
-10.522553	-1.839431	0.515494	0.002062	0.716757
-10.053747	-1.922556	0.520499	0.001975	0.716758
-9.668503	-1.989100	0.525504	0.001903	0.716763
-10.315734	-1.877292	0.530509	0.002023	0.716757
-10.372286	-1.937064	0.535514	0.002034	0.716619
-11.264580	-1.862379	0.540518	0.002200	0.716452
-11.017515	-1.905533	0.545523	0.002153	0.716454
-10.908697	-1.925086	0.550528	0.002133	0.716454
-11.117895	-1.891026	0.555533	0.002172	0.716449
-10.899731	-1.925485	0.560538	0.002131	0.716458
-11.270220	-1.862142	0.565542	0.002200	0.716453
-11.438199	-1.900615	0.570547	0.002231	0.716318
-11.937428	-1.901266	0.575552	0.002323	0.716141
-12.059878	-1.881908	0.580557	0.002346	0.716136
-12.388347	-1.820413	0.585562	0.002407	0.716143
-12.265765	-1.846477	0.590566	0.002384	0.716135
-11.980123	-1.895402	0.595571	0.002330	0.716139
-12.180671	-1.856852	0.600576	0.002367	0.716145
-12.268401	-1.845964	0.605581	0.002384	0.716136
-12.294200	-1.949714	0.610586	0.002388	0.715922
-13.116509	-1.819586	0.615590	0.002541	0.715890
-13.240746	-1.797545	0.620595	0.002564	0.715890
-12.751992	-1.883717	0.625600	0.002473	0.715892
-13.021835	-1.838613	0.630605	0.002523	0.715887
-12.772216	-1.878917	0.635610	0.002476	0.715895
-12.628696	-1.910206	0.640614	0.002449	0.715884
-13.378771	-1.935367	0.645619	0.002589	0.715570
-13.981698	-1.834467	0.650624	0.002701	0.715558
-14.299502	-1.783061	0.655629	0.002760	0.715548
-13.619984	-1.897865	0.660634	0.002633	0.715561
-13.714449	-1.885379	0.665638	0.002650	0.715552
-13.959635	-1.842342	0.670643	0.002696	0.715552
-13.881644	-1.852902	0.675648	0.002681	0.715559
-14.303444	-1.883535	0.680653	0.002759	0.715349
-15.022686	-1.806652	0.685658	0.002893	0.715248
-14.532054	-1.898082	0.690662	0.002801	0.715240
-14.615531	-1.884994	0.695667	0.002817	0.715237
-14.771440	-1.854870	0.700672	0.002846	0.715242
-14.864108	-1.842230	0.705677	0.002863	0.715235
-14.529658	-1.897928	0.710682	0.002800	0.715243
-14.888703	-1.927496	0.715686	0.002867	0.715058
-16.081391	-1.788191	0.720691	0.003089	0.714913
-15.404056	-1.906708	0.725696	0.002962	0.714918
-15.732466	-1.851124	0.730701	0.003023	0.714913
-15.807031	-1.834627	0.735706	0.003037	0.714919
-15.687282	-1.858726	0.740710	0.003014	0.714914
-15.562926	-1.882662	0.745715	0.002991	0.714911
-15.760903	-1.881698	0.750720	0.003028	0.714844
-16.853547	-1.804890	0.755725	0.003231	0.714610
-16.327355	-1.894754	0.760730	0.003133	0.714618
-16.503988	-1.866482	0.765734	0.003165	0.714612
-16.551414	-1.856866	0.770739	0.003174	0.714615
-16.343294	-1.893169	0.775744	0.003135	0.714617
-16.763892	-1.820884	0.780749	0.003213	0.714612
-16.766484	-1.817447	0.785754	0.003213	0.714618
-17.071101	-1.930581	0.790758	0.003270	0.714286
-17.652248	-1.829729	0.795763	0.003378	0.714281
-17.593775	-1.838390	0.800768	0.003367	0.714285
-17.646543	-1.832027	0.805773	0.003376	0.714280
-17.402898	-1.872303	0.810778	0.003331	0.714286
-17.654092	-1.829842	0.815782	0.003377	0.714282
-17.816804	-1.800394	0.820787	0.003407	0.714284
-17.497923	-1.929707	0.825792	0.003348	0.714140
-18.629547	-1.814405	0.830797	0.003558	0.713969
-18.365351	-1.856735	0.835802	0.003509	0.713979
-18.483487	-1.840452	0.840806	0.003531	0.713970
-18.392717	-1.854005	0.845811	0.003513	0.713975
-18.038880	-1.915369	0.850816	0.003447	0.713979
-18.713813	-1.798551	0.855821	0.003573	0.713973
-18.447467	-1.900565	0.860826	0.003523	0.713865
-19.329688	-1.847483	0.865830	0.003687	0.713658
-19.207764	-1.870671	0.870835	0.003664	0.713656
-19.051751	-1.896203	0.875840	0.003635	0.713660
-19.313585	-1.853530	0.880845	0.003683	0.713653
-19.416075	-1.830375	0.885850	0.003702	0.713663
-19.395878	-1.838029	0.890854	0.003698	0.713655
-19.278240	-1.894213	0.895859	0.003676	0.713586
-19.990747	-1.877013	0.900864	0.003809	0.713368
-20.350659	-1.817216	0.905869	0.003875	0.713360
-20.129992	-1.851012	0.910874	0.003834	0.713371
-19.916939	-1.892595	0.915878	0.003794	0.713364
-20.371002	-1.810804	0.920883	0.003879	0.713367
-20.239745	-1.831417	0.925888	0.003854	0.713373
-20.162923	-1.871917	0.930893	0.003839	0.713320
-20.874487	-1.890964	0.935898	0.003972	0.713030
-21.186861	-1.837947	0.940902	0.004030	0.713025
-21.297662	-1.817708	0.945907	0.004050	0.713026
-20.892636	-1.885846	0.950912	0.003974	0.713035
-21.077829	-1.859177	0.955917	0.004009	0.713023
-20.953167	-1.876028	0.960922	0.003985	0.713034
-20.654010	-1.951188	0.965926	0.003929	0.712991
-21.903466	-1.867305	0.970931	0.004162	0.712715
-21.890470	-1.867399	0.975936	0.004159	0.712720
-22.031503	-1.843733	0.980941	0.004185	0.712717
-22.049036	-1.837721	0.985946	0.004188	0.712723
-22.057157	-1.840521	0.990950	0.004189	0.712715
-22.078684	-1.836972	0.995955	0.004193	0.712715
-21.966566	-1.854375	1.000960	0.004172	0.712721
-22.945087	-1.822429	1.005965	0.004354	0.712438
-23.272743	-1.785493	1.010970	0.004415	0.712395
-22.961913	-1.842537	1.015974	0.004357	0.712392
-23.203210	-1.801004	1.020979	0.004402	0.712390
-23.097230	-1.816923	1.025984	0.004382	0.712396
-22.919735	-1.854636	1.030989	0.004348	0.712385
-22.788423	-1.873893	1.035994	0.004324	0.712393
-23.208074	-1.801835	1.040998	0.004402	0.712388
-23.541938	-1.891538	1.046003	0.004464	0.712091
-23.348842	-1.922668	1.051008	0.004427	0.712098
-24.204645	-1.773322	1.056013	0.004586	0.712093
-23.744196	-1.850719	1.061018	0.004501	0.712102
-23.635624	-1.874857	1.066022	0.004480	0.712093
-24.167565	-1.780947	1.071027	0.004579	0.712092
-23.929489	-1.820562	1.076032	0.004534	0.712098
-24.328723	-1.905129	1.081037	0.004609	0.711788
-24.767403	-1.837035	1.086042	0.004690	0.711768
-24.918519	-1.811490	1.091046	0.004718	0.711766
-24.743926	-1.844219	1.096051	0.004685	0.711763
-24.694597	-1.849969	1.101056	0.004676	0.711769
-25.131843	-1.776884	1.106061	0.004757	0.711760
-24.962426	-1.803445	1.111066	0.004725	0.711768
-24.685433	-1.922414	1.116070	0.004673	0.711630
-25.913224	-1.792362	1.121075	0.004902	0.711453
-25.679241	-1.830274	1.126080	0.004858	0.711461
-25.887706	-1.795918	1.131085	0.004897	0.711456
-25.628184	-1.837403	1.136090	0.004848	0.711466
-25.787047	-1.812121	1.141094	0.004877	0.711460
-25.885907	-1.795652	1.146099	0.004896	0.711458
-25.646626	-1.862564	1.151104	0.004851	0.711410
-26.553990	-1.838628	1.156109	0.005020	0.711136
-26.332940	-1.874238	1.161114	0.004978	0.711144
-26.649501	-1.818114	1.166118	0.005037	0.711144
-26.783805	-1.794899	1.171123	0.005062	0.711143
-26.865837	-1.778417	1.176128	0.005077	0.711147
-26.650293	-1.821259	1.181133	0.005036	0.711138
-26.346036	-1.870601	1.186138	0.004980	0.711148
-27.017787	-1.882614	1.191142	0.005104	0.710886
-27.635518	-1.780210	1.196147	0.005219	0.710871
-27.085034	-1.873238	1.201152	0.005117	0.710882
-27.280186	-1.843674	1.206157	0.005153	0.710872
-27.351856	-1.825364	1.211162	0.005166	0.710883
-27.221228	-1.851236	1.216166	0.005141	0.710878
-27.374689	-1.871558	1.221171	0.005170	0.710784
-28.335444	-1.818865	1.226176	0.005348	0.710547
-28.161141	-1.855880	1.231181	0.005316	0.710536
-28.355801	-1.817296	1.236186	0.005352	0.710544
-28.407393	-1.811203	1.241190	0.005361	0.710538
-28.477604	-1.797962	1.246195	0.005374	0.710540
-28.111060	-1.861419	1.251200	0.005305	0.710544
-28.323495	-1.860541	1.256205	0.005345	0.710471
-29.138675	-1.838927	1.261210	0.005496	0.710224
-29.105046	-1.846340	1.266214	0.005490	0.710222
-29.431821	-1.790072	1.271219	0.005550	0.710218
-29.136888	-1.838075	1.276224	0.005495	0.710228
-29.161850	-1.839343	1.281229	0.005500	0.710217
-29.152161	-1.837099	1.286234	0.005498	0.710225
-29.094191	-1.870449	1.291238	0.005487	0.710179
-30.262675	-1.804946	1.296243	0.005704	0.709895
-29.916595	-1.861834	1.301248	0.005639	0.709905
-30.109596	-1.833347	1.306253	0.005675	0.709893
-30.170165	-1.818584	1.311258	0.005686	0.709902
-30.023508	-1.846842	1.316262	0.005659	0.709898
-30.289928	-1.801953	1.321267	0.005708	0.709893
-30.303872	-1.795148	1.326272	0.005710	0.709902
-30.556461	-1.863072	1.331277	0.005757	0.709677
-31.153188	-1.795100	1.336282	0.005868	0.709600
-30.941759	-1.832014	1.341286	0.005829	0.709602
-31.345099	-1.763384	1.346291	0.005903	0.709596
-31.260601	-1.775062	1.351296	0.005887	0.709603
-31.144248	-1.799987	1.356301	0.005866	0.709595
-31.274866	-1.773640	1.361306	0.005890	0.709602
-31.110212	-1.835346	1.366310	0.005859	0.709538
-31.630713	-1.880385	1.371315	0.005956	0.709262
-31.573213	-1.886239	1.376320	0.005945	0.709272
-32.253209	-1.770251	1.381325	0.006071	0.709262
-31.851830	-1.838757	1.386330	0.005996	0.709268
-31.835791	-1.842136	1.391334	0.005993	0.709267
-32.434304	-1.737276	1.396339	0.006104	0.709264
-31.687700	-1.906661	1.401344	0.005965	0.709192
-32.594921	-1.862668	1.406349	0.006134	0.708957
-32.932682	-1.799131	1.411354	0.006196	0.708964
-32.984772	-1.791304	1.416358	0.006206	0.708961
-32.823161	-1.823864	1.421363	0.006175	0.708954
-32.911139	-1.804572	1.426368	0.006191	0.708962
-33.350093	-1.731226	1.431373	0.006273	0.708953
-32.704877	-1.843349	1.436378	0.006153	0.708959
-33.102453	-1.922763	1.441382	0.006227	0.708658
-33.835355	-1.803687	1.446387	0.006363	0.708636
-33.627638	-1.837254	1.451392	0.006324	0.708643
-33.475787	-1.868502	1.456397	0.006295	0.708635
-33.940389	-1.782827	1.461402	0.006382	0.708641
-33.975273	-1.776779	1.466406	0.006388	0.708641
-33.715375	-1.823699	1.471411	0.006339	0.708640
-34.010780	-1.902164	1.476416	0.006394	0.708378
-34.897762	-1.760176	1.481421	0.006559	0.708346
-34.581714	-1.812742	1.486426	0.006500	0.708354
-34.397867	-1.846342	1.491430	0.006465	0.708353
-35.026682	-1.737708	1.496435	0.006582	0.708346
-34.565894	-1.814046	1.501440	0.006496	0.708359
-34.363969	-1.855230	1.506445	0.006459	0.708349
-34.933767	-1.901746	1.511450	0.006564	0.708052
-35.832662	-1.759959	1.516454	0.006732	0.708016
-35.481812	-1.825817	1.521459	0.006666	0.708009
-35.245685	-1.864414	1.526464	0.006622	0.708017
-35.780021	-1.772266	1.531469	0.006721	0.708011
-35.633063	-1.794969	1.536474	0.006693	0.708018
-35.146419	-1.880943	1.541478	0.006603	0.708020
-36.039980	-1.856874	1.546483	0.006769	0.707750
-36.432252	-1.807556	1.551488	0.006842	0.707709
-36.314548	-1.833959	1.556493	0.006820	0.707698
-36.201515	-1.850968	1.561498	0.006798	0.707705
-36.472209	-1.803084	1.566502	0.006848	0.707705
-36.474007	-1.805696	1.571507	0.006849	0.707699
-36.254471	-1.840132	1.576512	0.006807	0.707709
-36.985715	-1.839250	1.581517	0.006943	0.707450
-37.750262	-1.734845	1.586522	0.007085	0.707386
-37.218195	-1.832342	1.591526	0.006986	0.707381
-37.351505	-1.810812	1.596531	0.007011	0.707377
-37.318406	-1.811825	1.601536	0.007004	0.707388
-37.307176	-1.819209	1.606541	0.007002	0.707377
-37.187667	-1.837258	1.611546	0.006980	0.707384
-37.177552	-1.903286	1.616550	0.006978	0.707256
-38.262065	-1.797358	1.621555	0.007179	0.707081
-37.869946	-1.863146	1.626560	0.007106	0.707089
-38.483362	-1.756814	1.631565	0.007220	0.707084
-38.271287	-1.792803	1.636570	0.007180	0.707088
-37.875647	-1.862601	1.641574	0.007107	0.707090
-38.459131	-1.761176	1.646579	0.007215	0.707085
-38.560258	-1.785850	1.651584	0.007234	0.707000
-39.272122	-1.782062	1.656589	0.007366	0.706753
-38.911886	-1.844269	1.661594	0.007299	0.706757
-39.138530	-1.802990	1.666598	0.007341	0.706759
-39.278849	-1.781140	1.671603	0.007366	0.706753
-38.941753	-1.836735	1.676608	0.007303	0.706763
-39.332523	-1.772340	1.681613	0.007376	0.706753
-39.128466	-1.809933	1.686618	0.007338	0.706751
-39.621583	-1.871931	1.691622	0.007429	0.706450
-40.098230	-1.790864	1.696627	0.007518	0.706443
-40.267428	-1.756252	1.701632	0.007549	0.706452
-39.861120	-1.834170	1.706637	0.007473	0.706441
-40.068739	-1.794301	1.711642	0.007512	0.706448
-40.420765	-1.729972	1.716646	0.007577	0.706451
-40.263954	-1.760775	1.721651	0.007548	0.706446
-39.770217	-1.938475	1.726656	0.007456	0.706266
-41.273151	-1.739417	1.731661	0.007735	0.706128
-41.269745	-1.737632	1.736666	0.007734	0.706133
-40.879447	-1.806134	1.741670	0.007661	0.706136
-41.414613	-1.713390	1.746675	0.007761	0.706131
-41.034840	-1.777415	1.751680	0.007690	0.706139
-41.131063	-1.766178	1.756685	0.007708	0.706127
-40.840857	-1.836094	1.761690	0.007653	0.706091
-41.721190	-1.790110	1.766694	0.007817	0.705868
-41.841422	-1.771835	1.771699	0.007839	0.705862
-41.602195	-1.809101	1.776704	0.007794	0.705874
-41.808378	-1.776397	1.781709	0.007833	0.705866
-41.883109	-1.762896	1.786714	0.007846	0.705867
-41.419838	-1.844913	1.791718	0.007760	0.705868
-41.620593	-1.888688	1.796723	0.007797	0.705709
-42.801746	-1.765467	1.801728	0.008017	0.705533
-42.484492	-1.827702	1.806733	0.007957	0.705522
-42.722884	-1.782310	1.811738	0.008002	0.705529
-42.818152	-1.764061	1.816742	0.008019	0.705532
-42.733803	-1.782837	1.821747	0.008003	0.705525
-42.411977	-1.835762	1.826752	0.007943	0.705534
-43.006338	-1.807622	1.831757	0.008054	0.705378
-44.066181	-1.697954	1.836762	0.008251	0.705219
-43.328545	-1.831330	1.841766	0.008113	0.705215
-43.569950	-1.790790	1.846771	0.008158	0.705211
-43.535055	-1.793149	1.851776	0.008151	0.705219
-43.462075	-1.810090	1.856781	0.008137	0.705211
-43.416962	-1.816248	1.861786	0.008129	0.705216
-43.423604	-1.885983	1.866790	0.008130	0.705073
-44.700044	-1.749674	1.871795	0.008367	0.704890
-43.842200	-1.898902	1.876800	0.008207	0.704898
-44.298954	-1.822217	1.881805	0.008292	0.704889
-44.697584	-1.748259	1.886810	0.008366	0.704895
-44.163135	-1.843515	1.891814	0.008266	0.704895
-44.495509	-1.788500	1.896819	0.008328	0.704887
-44.614759	-1.856062	1.901824	0.008350	0.704709
-45.489166	-1.759071	1.906829	0.008513	0.704590
-45.191240	-1.809876	1.911834	0.008457	0.704595
-44.999120	-1.843639	1.916838	0.008421	0.704597
-45.409610	-1.773880	1.921843	0.008497	0.704590
-44.957153	-1.850028	1.926848	0.008413	0.704600
-45.130679	-1.823135	1.931853	0.008445	0.704592
-45.794085	-1.840111	1.936858	0.008568	0.704320
-46.181016	-1.798323	1.941862	0.008640	0.704266
-46.033024	-1.828478	1.946867	0.008612	0.704258
-45.739435	-1.876189	1.951872	0.008557	0.704268
-46.259423	-1.785938	1.956877	0.008654	0.704264
-46.129386	-1.807860	1.961882	0.008629	0.704267
-45.963872	-1.836570	1.966886	0.008598	0.704269
-46.915262	-1.821214	1.971891	0.008775	0.703958
-46.770635	-1.844886	1.976896	0.008748	0.703963
-46.900664	-1.825937	1.981901	0.008772	0.703955
-47.186304	-1.773401	1.986906	0.008825	0.703958
-47.185837	-1.770985	1.991910	0.008825	0.703964
-47.019687	-1.806621	1.996915	0.008794	0.703952
-47.143556	-1.835258	2.001920	0.008816	0.703850

-47.804010	-1.818867	2.011917	0.008939	0.703646
-48.021348	-1.784718	2.021914	0.008979	0.703638
-47.758386	-1.831477	2.031910	0.008930	0.703639
-47.806623	-1.823913	2.041907	0.008938	0.703638
-47.945776	-1.798398	2.051904	0.008964	0.703640
-47.890020	-1.809375	2.061901	0.008953	0.703639
-47.942727	-1.798653	2.071898	0.008962	0.703642
-47.838638	-1.819371	2.081894	0.008942	0.703639
-48.056059	-1.780249	2.091891	0.008982	0.703640
-47.793367	-1.828742	2.101888	0.008933	0.703638
-47.041123	-1.812315	2.111885	0.008793	0.703943
-47.091893	-1.794846	2.121882	0.008802	0.703960
-46.867327	-1.835998	2.131878	0.008759	0.703959
-47.048663	-1.805480	2.141875	0.008793	0.703956
-47.143698	-1.786435	2.151872	0.008810	0.703961
-47.111280	-1.794260	2.161869	0.008803	0.703958
-46.485922	-1.780023	2.171866	0.008687	0.704212
-46.114347	-1.820094	2.181862	0.008617	0.704266
-46.226021	-1.800718	2.191859	0.008637	0.704266
-45.967170	-1.845927	2.201856	0.008589	0.704268
-45.993655	-1.787308	2.211853	0.008593	0.704378
-45.267286	-1.808296	2.221850	0.008458	0.704597
-45.202572	-1.820056	2.231846	0.008445	0.704598
-45.368098	-1.791002	2.241843	0.008475	0.704598
-45.169993	-1.785546	2.251840	0.008438	0.704681
-44.405333	-1.815598	2.261837	0.008295	0.704896
-44.475726	-1.804047	2.271834	0.008308	0.704894
-44.490596	-1.802900	2.281830	0.008310	0.704892
-44.226093	-1.750544	2.291827	0.008261	0.705094
-43.541614	-1.811422	2.301824	0.008133	0.705217
-43.560588	-1.808845	2.311821	0.008136	0.705217
-43.598870	-1.799992	2.321818	0.008142	0.705222
-42.718209	-1.804728	2.331814	0.007978	0.705529
-42.663552	-1.812908	2.341811	0.007967	0.705533
-42.446386	-1.851728	2.351808	0.007927	0.705533
-42.637576	-1.769200	2.361805	0.007962	0.705632
-41.766858	-1.807663	2.371802	0.007799	0.705868
-41.612686	-1.836418	2.381798	0.007770	0.705866
-41.767019	-1.807847	2.391795	0.007798	0.705869
-41.223589	-1.825664	2.401792	0.007697	0.706029
-41.003117	-1.813181	2.411789	0.007655	0.706134
-41.118398	-1.791726	2.421786	0.007676	0.706136
-41.091361	-1.763025	2.431782	0.007671	0.706204
-40.544000	-1.738374	2.441779	0.007568	0.706451
-40.056825	-1.825167	2.451776	0.007477	0.706452
-40.426480	-1.747595	2.461773	0.007546	0.706476
-39.679701	-1.740854	2.471770	0.007406	0.706758
-39.399201	-1.791816	2.481766	0.007354	0.706757
-39.305460	-1.809021	2.491763	0.007336	0.706757
-38.829037	-1.763641	2.501760	0.007246	0.707019
-38.594189	-1.770147	2.511757	0.007202	0.707091
-38.441878	-1.800633	2.521754	0.007174	0.707085
-38.476697	-1.731152	2.531750	0.007180	0.707213
-37.645694	-1.795621	2.541747	0.007024	0.707382
-37.480713	-1.823927	2.551744	0.006993	0.707385
-37.614880	-1.800079	2.561741	0.007018	0.707385
-36.906399	-1.783079	2.571738	0.006885	0.707674
-37.050256	-1.740517	2.581734	0.006912	0.707709
-36.974441	-1.753746	2.591731	0.006897	0.707710
-36.413511	-1.756525	2.601728	0.006792	0.707906
-36.186919	-1.738823	2.611725	0.006750	0.708023
-36.000291	-1.773479	2.621722	0.006715	0.708021
-36.187907	-1.680030	2.631718	0.006749	0.708142
-35.122991	-1.762237	2.641715	0.006550	0.708359
-34.880596	-1.805857	2.651712	0.006505	0.708359
-35.206275	-1.749085	2.661709	0.006565	0.708357
-34.258635	-1.786591	2.671706	0.006388	0.708621
-34.190450	-1.787729	2.681702	0.006375	0.708644
-34.065614	-1.808718	2.691699	0.006351	0.708647
-34.107129	-1.760530	2.701696	0.006359	0.708730
-33.408213	-1.767996	2.711693	0.006228	0.708965
-33.428612	-1.765871	2.721690	0.006231	0.708963
-33.718393	-1.713939	2.731686	0.006285	0.708964
-32.659187	-1.750701	2.741683	0.006087	0.709269
-32.385576	-1.798007	2.751680	0.006036	0.709273
-32.609861	-1.759819	2.761677	0.006077	0.709270
-32.064303	-1.766302	2.771674	0.005975	0.709453
-31.742294	-1.748979	2.781670	0.005915	0.709603
-31.757014	-1.748570	2.791667	0.005917	0.709600
-31.664827	-1.746036	2.801664	0.005899	0.709638
-30.970423	-1.739202	2.811661	0.005770	0.709900
-30.744554	-1.779091	2.821658	0.005727	0.709902
-31.037512	-1.729018	2.831654	0.005781	0.709898
-30.252528	-1.745275	2.841651	0.005635	0.710146
-29.946844	-1.761257	2.851648	0.005577	0.710224
-29.892369	-1.771461	2.861645	0.005567	0.710224
-29.757491	-1.765838	2.871642	0.005541	0.710284
-29.289765	-1.722000	2.881638	0.005454	0.710539
-28.715120	-1.823805	2.891635	0.005346	0.710541
-29.078805	-1.759842	2.901632	0.005414	0.710540
-28.561270	-1.736142	2.911629	0.005317	0.710773
-28.270881	-1.735542	2.921626	0.005262	0.710878
-28.153099	-1.757300	2.931622	0.005240	0.710877
-28.013027	-1.756175	2.941619	0.005213	0.710930
-27.530652	-1.734521	2.951616	0.005123	0.711146
-27.316271	-1.771848	2.961613	0.005083	0.711148
-27.471156	-1.744979	2.971610	0.005111	0.711148
-27.085622	-1.677395	2.981606	0.005039	0.711420
-26.572432	-1.749004	2.991603	0.004943	0.711461
-26.506541	-1.758812	3.001600	0.004930	0.711465
-26.072582	-1.743962	3.011597	0.004849	0.711650
-25.725033	-1.747439	3.021594	0.004784	0.711768
-25.752755	-1.742407	3.031590	0.004789	0.711769
-25.649071	-1.730685	3.041587	0.004769	0.711830
-24.773277	-1.752632	3.051584	0.004605	0.712098
-24.493744	-1.801328	3.061581	0.004553	0.712101
-24.749585	-1.757335	3.071578	0.004600	0.712098
-24.403958	-1.735129	3.081574	0.004535	0.712266
-23.914800	-1.759349	3.091571	0.004444	0.712392
-24.024596	-1.738711	3.101568	0.004464	0.712395
-23.901413	-1.731533	3.111565	0.004440	0.712454
-23.183956	-1.727767	3.121562	0.004306	0.712717
-23.057184	-1.751361	3.131558	0.004282	0.712716
-23.105947	-1.743247	3.141555	0.004291	0.712716
-22.477676	-1.729820	3.151552	0.004174	0.712966
-22.011096	-1.780069	3.161549	0.004086	0.713032
-22.250888	-1.739136	3.171546	0.004130	0.713030
-22.121996	-1.718847	3.181542	0.004106	0.713116
-21.339891	-1.731966	3.191539	0.003960	0.713368
-21.171106	-1.763084	3.201536	0.003928	0.713367
-21.328204	-1.735432	3.211533	0.003957	0.713367
-20.843370	-1.702494	3.221530	0.003866	0.713605
-20.583109	-1.723340	3.231526	0.003817	0.713657
-20.452719	-1.748285	3.241523	0.003793	0.713654
-20.162874	-1.737839	3.251520	0.003738	0.713779
-19.363717	-1.781238	3.261517	0.003589	0.713976
-19.753340	-1.713143	3.271514	0.003661	0.713974
-19.527795	-1.754294	3.281510	0.003619	0.713973
-18.878895	-1.731593	3.291507	0.003497	0.714249
-18.867452	-1.714849	3.301504	0.003495	0.714287
-18.463826	-1.787884	3.311501	0.003419	0.714286
-18.610905	-1.696743	3.321498	0.003446	0.714416
-17.535490	-1.790204	3.331494	0.003245	0.714611
-17.833501	-1.737371	3.341491	0.003300	0.714612
-17.676800	-1.764249	3.351488	0.003271	0.714614
-17.098307	-1.753124	3.361485	0.003163	0.714842
-17.099198	-1.717037	3.371482	0.003162	0.714914
-16.910632	-1.752386	3.381478	0.003127	0.714911
-17.011773	-1.674766	3.391475	0.003145	0.715031
-15.929600	-1.764842	3.401472	0.002943	0.715235
-16.101045	-1.733101	3.411469	0.002975	0.715238
-15.996536	-1.754027	3.421466	0.002955	0.715235
-15.439547	-1.713188	3.431462	0.002851	0.715513
-15.375978	-1.707074	3.441459	0.002839	0.715549
-15.114592	-1.752281	3.451456	0.002789	0.715552
-14.988495	-1.692851	3.461453	0.002765	0.715715
-14.343920	-1.720793	3.471450	0.002645	0.715888
-14.205985	-1.747044	3.481446	0.002619	0.715886
-14.257102	-1.740129	3.491443	0.002628	0.715882
-13.318199	-1.788527	3.501440	0.002453	0.716119
-13.476276	-1.751080	3.511437	0.002482	0.716138
-13.443839	-1.756486	3.521434	0.002475	0.716139
-13.456339	-1.692931	3.531430	0.002477	0.716262
-12.651025	-1.740907	3.541427	0.002327	0.716452
-12.556518	-1.756304	3.551424	0.002309	0.716455
-12.602461	-1.747748	3.561421	0.002317	0.716457
-11.809638	-1.737403	3.571418	0.002169	0.716758
-11.708484	-1.755127	3.581414	0.002150	0.716759
-11.674349	-1.762019	3.591411	0.002143	0.716758
-11.449922	-1.719720	3.601408	0.002101	0.716922
-10.474311	-1.808873	3.611405	0.001918	0.717090
-10.460738	-1.814157	3.621402	0.001916	0.717085
-10.346753	-1.834837	3.631398	0.001894	0.717085
-10.148548	-1.808451	3.641395	0.001857	0.717208
-9.204607	-1.888761	3.651392	0.001680	0.717383
-9.609924	-1.817181	3.661389	0.001755	0.717382
-9.344227	-1.863738	3.671386	0.001705	0.717385
-9.310379	-1.803107	3.681382	0.001699	0.717517
-8.228638	-1.900564	3.691379	0.001497	0.717706
-8.195639	-1.906186	3.701376	0.001490	0.717708
-8.212873	-1.902466	3.711373	0.001493	0.717710
-8.092112	-1.923997	3.721370	0.001470	0.717711
-7.463947	-1.878649	3.731366	0.001353	0.718022
-7.294126	-1.910420	3.741363	0.001321	0.718020
-7.272105	-1.915353	3.751360	0.001316	0.718019
-7.422047	-1.887244	3.761357	0.001344	0.718022
-6.503032	-1.885512	3.771354	0.001172	0.718350
-6.426688	-1.896597	3.781350	0.001157	0.718356
-6.146038	-1.946446	3.791347	0.001105	0.718357
-6.297172	-1.919509	3.801344	0.001133	0.718358
-5.630883	-1.905386	3.811341	0.001008	0.718621
-5.178839	-1.974633	3.821338	0.000923	0.718644
-5.355297	-1.943939	3.831334	0.000956	0.718643
-5.481613	-1.920275	3.841331	0.000979	0.718646
-4.767760	-1.893451	3.851328	0.000846	0.718951
-4.465845	-1.941697	3.861325	0.000789	0.718963
-4.410100	-1.951408	3.871322	0.000778	0.718964
-4.737999	-1.847709	3.881318	0.000839	0.719054
-3.438402	-1.968034	3.891315	0.000596	0.719274
-3.745122	-1.912675	3.901312	0.000653	0.719276
-3.578806	-1.943228	3.911309	0.000622	0.719275
-3.182988	-1.901128	3.921306	0.000547	0.719498
-2.941491	-1.890473	3.931302	0.000502	0.719605
-2.730108	-1.928416	3.941299	0.000462	0.719605
-2.731173	-1.912505	3.951296	0.000462	0.719637
-2.479403	-1.820533	3.961293	0.000415	0.719907
-1.770807	-1.947857	3.971290	0.000282	0.719906
-2.136397	-1.884436	3.981286	0.000350	0.719903
-1.795815	-1.810250	3.991283	0.000286	0.720170
-1.350490	-1.859177	4.001280	0.000203	0.720230
-1.706262	-1.796395	4.011277	0.000268	0.720230
-1.116072	-1.775290	4.021274	0.000158	0.720479
-1.294995	-1.710534	4.031270	0.000191	0.720545
-1.106332	-1.727037	4.041267	0.000155	0.720579
-1.064493	-1.579857	4.051264	0.000147	0.720884
-1.224546	-1.549587	4.061261	0.000176	0.720889
-0.926349	-1.498975	4.071258	0.000120	0.721093
-1.103156	-1.450264	4.081254	0.000153	0.721128
-0.511337	-1.419266	4.091251	0.000042	0.721397
-0.697009	-1.363285	4.101248	0.000076	0.721443
-0.763729	-1.210943	4.111245	0.000088	0.721720
-0.744375	-1.163420	4.121242	0.000084	0.721821
-0.602842	-1.058074	4.131238	0.000057	0.722078
-0.756146	-0.938790	4.141235	0.000085	0.722260
-0.550637	-0.890379	4.151232	0.000047	0.722427
-0.222931	-0.810225	4.161229	-0.000015	0.722700
-0.154313	-0.713286	4.171226	-0.000028	0.722915
-0.204285	-0.607432	4.181222	-0.000019	0.723106
-0.150422	-0.493734	4.191219	-0.000030	0.723349
-0.131559	-0.353825	4.201216	-0.000034	0.723630
-0.434398	-0.179760	4.211213	0.000022	0.723866
-0.141337	-0.096307	4.221210	-0.000033	0.724133
-0.074137	0.031719	4.231206	-0.000046	0.724408
0.117618	0.135549	4.241203	-0.000082	0.724679
0.000000	0.338545	4.251200	-0.000061	0.725036

0.165144	0.932937	4.256205	-0.000092	0.726255
0.433841	2.156024	4.261210	-0.000144	0.728733
0.553404	4.009686	4.266214	-0.000167	0.732373
0.754685	6.384839	4.271219	-0.000206	0.737028
1.025088	9.271534	4.276224	-0.000259	0.742653
1.376288	12.617191	4.281229	-0.000327	0.749134
1.670485	16.430094	4.286234	-0.000384	0.756415
2.299381	20.586996	4.291238	-0.000504	0.764377
2.745908	25.185069	4.296243	-0.000591	0.773006
3.271878	30.139068	4.301248	-0.000692	0.782211
4.099814	35.383639	4.306253	-0.000850	0.791925
4.962345	40.952874	4.311258	-0.001014	0.802105
5.625062	46.866924	4.316262	-0.001142	0.812698
6.019123	53.105454	4.321267	-0.001219	0.823632
6.844708	59.555995	4.326272	-0.001377	0.834911
7.607114	66.220599	4.331277	-0.001524	0.846380
9.886415	72.884414	4.336282	-0.001953	0.858135
11.415138	79.881986	4.341286	-0.002242	0.870059
11.784388	87.267838	4.346291	-0.002316	0.882117
12.558020	94.768732	4.351296	-0.002465	0.894307
13.523812	102.372106	4.356301	-0.002650	0.906546
14.305116	110.176178	4.361306	-0.002801	0.918881
15.040806	118.096337	4.366310	-0.002943	0.931217
15.916293	126.102797	4.371315	-0.003112	0.943557
16.944018	134.200702	4.376320	-0.003309	0.955913
17.425110	142.460436	4.381325	-0.003404	0.968207
18.024541	150.796392	4.386330	-0.003521	0.980487
18.686882	159.200267	4.391334	-0.003650	0.992728
19.240821	167.644100	4.396339	-0.003759	1.004849
20.013619	176.111188	4.401344	-0.003909	1.016910
20.463519	184.659816	4.406349	-0.003998	1.028865
21.169726	193.204078	4.411354	-0.004136	1.040736
21.558237	201.828125	4.416358	-0.004214	1.052507
22.118249	210.434774	4.421363	-0.004324	1.064164
22.975884	219.036506	4.426368	-0.004489	1.075755
23.317052	227.686679	4.431373	-0.004559	1.087169
23.780086	236.350531	4.436378	-0.004651	1.098509
24.389413	244.988914	4.441382	-0.004770	1.109733
24.887628	253.640600	4.446387	-0.004869	1.120837
25.328205	262.306924	4.451392	-0.004957	1.131837
25.812676	270.946645	4.456397	-0.005053	1.142707
26.574918	279.584294	4.461402	-0.005201	1.153531
27.052805	288.216087	4.466406	-0.005295	1.164187
27.307487	296.873493	4.471411	-0.005349	1.174732
27.967710	305.454010	4.476416	-0.005477	1.185173
28.372174	314.071161	4.481421	-0.005559	1.195514
28.600910	322.684415	4.486426	-0.005607	1.205727
29.402243	331.213737	4.491430	-0.005762	1.215869
29.700667	339.798854	4.496435	-0.005823	1.225893
30.191452	348.374009	4.501440	-0.005920	1.235862
30.683768	356.880920	4.506445	-0.006018	1.245673
31.244880	365.402438	4.511450	-0.006128	1.255437
31.781256	373.899003	4.516454	-0.006234	1.265092
31.939562	382.456915	4.521459	-0.006269	1.274672
32.569158	390.907529	4.526464	-0.006392	1.284149
32.945544	399.407051	4.531469	-0.006468	1.293563
33.292359	407.888352	4.536474	-0.006538	1.302884
33.921753	416.402627	4.541478	-0.006661	1.312226
34.343031	424.868866	4.546483	-0.006745	1.321412
34.792563	433.283914	4.551488	-0.006835	1.330485
34.994361	441.718335	4.556493	-0.006878	1.339473
35.579576	450.077929	4.561498	-0.006993	1.348389
35.987998	458.479345	4.566502	-0.007074	1.357260
36.861376	466.759667	4.571507	-0.007243	1.366028
37.603731	475.112028	4.576512	-0.007387	1.374791
37.780010	483.518951	4.581517	-0.007425	1.383458
37.760012	491.976285	4.586522	-0.007427	1.392089
38.207320	500.306241	4.591526	-0.007516	1.400616
38.848351	508.596167	4.596531	-0.007641	1.409083
39.287527	516.950684	4.601536	-0.007728	1.417531
39.916510	525.229510	4.606541	-0.007851	1.425885
40.433213	533.567536	4.611546	-0.007953	1.434230
40.866329	541.879544	4.616550	-0.008039	1.442487
41.042146	550.221955	4.621555	-0.008078	1.450685
41.520229	558.530052	4.626560	-0.008172	1.458852
41.878708	566.828457	4.631565	-0.008245	1.466946
42.330411	575.172269	4.636570	-0.008334	1.475052
43.785633	583.271640	4.641574	-0.008611	1.483038
44.552332	591.513662	4.646579	-0.008759	1.491010
44.931486	599.834945	4.651584	-0.008835	1.498953
45.319980	608.117050	4.656589	-0.008913	1.506819
45.640500	616.431383	4.661594	-0.008979	1.514664
46.141107	624.683311	4.666598	-0.009078	1.522437
46.598983	632.936663	4.671603	-0.009168	1.530166
47.141878	641.203323	4.676608	-0.009275	1.537881
47.288464	649.483165	4.681613	-0.009308	1.545510
47.606647	657.777572	4.686618	-0.009373	1.553140
47.904246	666.024013	4.691622	-0.009434	1.560686
48.216492	674.252944	4.696627	-0.009498	1.568182
49.040697	682.422738	4.701632	-0.009657	1.575664
49.518231	690.626503	4.706637	-0.009751	1.583090
50.033561	698.853508	4.711642	-0.009853	1.590507
50.479020	707.089424	4.716646	-0.009941	1.597888
50.849772	715.286998	4.721651	-0.010016	1.605190
51.663139	723.479650	4.726656	-0.010173	1.612517
52.469005	731.635335	4.731661	-0.010328	1.619777
53.049140	739.844423	4.736666	-0.010442	1.627020
53.819477	748.091027	4.741670	-0.010591	1.634289
54.236454	756.284553	4.746675	-0.010674	1.641431
54.710846	764.494406	4.751680	-0.010768	1.648564
55.130155	772.700793	4.756685	-0.010852	1.655656
55.661297	780.873957	4.761690	-0.010956	1.662704
56.355086	789.044818	4.766694	-0.011091	1.669742
56.896740	797.238292	4.771699	-0.011197	1.676749
57.572236	805.396096	4.776704	-0.011329	1.683715
58.201337	813.571928	4.781709	-0.011451	1.690660
58.509765	821.805430	4.786714	-0.011514	1.697583
59.149721	829.974941	4.791718	-0.011639	1.704468
59.565002	838.185301	4.796723	-0.011722	1.711329
60.053191	846.380866	4.801728	-0.011818	1.718160
60.432303	854.528231	4.806733	-0.011894	1.724910
60.888209	862.714593	4.811738	-0.011985	1.731676
61.387271	870.883970	4.816742	-0.012083	1.738407
61.840924	879.025517	4.821747	-0.012173	1.745083
62.490757	887.187369	4.826752	-0.012300	1.751775
62.833484	895.366855	4.831757	-0.012369	1.758416
63.194931	903.525491	4.836762	-0.012442	1.765019
63.706890	911.691034	4.841766	-0.012543	1.771620
63.954269	919.866399	4.846771	-0.012595	1.778173
64.473381	928.011079	4.851776	-0.012697	1.784710
64.869199	936.201741	4.856781	-0.012776	1.791244
65.332426	944.370063	4.861786	-0.012868	1.797745
65.721104	952.501195	4.866790	-0.012946	1.804184
66.054374	960.644994	4.871795	-0.013013	1.810604
66.557237	968.785647	4.876800	-0.013112	1.817019
67.181799	976.888556	4.881805	-0.013234	1.823396
67.557852	985.035723	4.886810	-0.013310	1.829755
67.715913	993.230571	4.891814	-0.013345	1.836103
68.260081	1001.317853	4.896819	-0.013452	1.842392
68.703573	1009.465668	4.901824	-0.013540	1.848694
68.826269	1017.652014	4.906829	-0.013568	1.854967
69.057766	1025.788197	4.911834	-0.013617	1.861193
69.623993	1033.903386	4.916838	-0.013728	1.867420
69.983131	1042.068726	4.921843	-0.013800	1.873641
70.328445	1050.190283	4.926848	-0.013870	1.879807
70.734806	1058.287954	4.931853	-0.013951	1.885941
70.981847	1066.444324	4.936858	-0.014003	1.892082
71.170944	1074.598347	4.941862	-0.014043	1.898193
71.547388	1082.699617	4.946867	-0.014119	1.904268
72.053540	1090.819267	4.951872	-0.014219	1.910351
72.317141	1098.967083	4.956877	-0.014273	1.916408
72.661910	1107.068674	4.961882	-0.014343	1.922421
73.309571	1115.151329	4.966886	-0.014469	1.928434
73.522220	1123.301871	4.971891	-0.014514	1.934431
73.796079	1131.430612	4.976896	-0.014571	1.940400
74.183063	1139.529222	4.981901	-0.014648	1.946341
74.436191	1147.720388	4.986906	-0.014701	1.952316
74.820781	1155.838575	4.991910	-0.014778	1.958234
75.226210	1163.890171	4.996915	-0.014859	1.964089
75.677363	1171.980615	5.001920	-0.014949	1.969959
75.674313	1180.142909	5.006925	-0.014953	1.975814
75.742032	1188.260095	5.011930	-0.014972	1.981628
76.170073	1196.349962	5.016934	-0.015057	1.987443
76.353065	1204.481870	5.021939	-0.015096	1.993245
76.550350	1212.598483	5.026944	-0.015139	1.999020
76.850532	1220.669101	5.031949	-0.015200	2.004758
77.256446	1228.763636	5.036954	-0.015281	2.010506
77.449515	1236.913395	5.041958	-0.015323	2.016255
77.705840	1244.999416	5.046963	-0.015376	2.021949
78.078834	1253.094384	5.051968	-0.015451	2.027646
78.273997	1261.240654	5.056973	-0.015493	2.033344
78.427621	1269.348143	5.061978	-0.015527	2.038995
78.967984	1277.390552	5.066982	-0.015633	2.044624
78.883102	1285.534422	5.071987	-0.015622	2.050245
79.204597	1293.635154	5.076992	-0.015688	2.055861
79.290813	1301.729300	5.081997	-0.015709	2.061434
79.684303	1309.804868	5.087002	-0.015788	2.067010
79.695701	1317.957875	5.092006	-0.015796	2.072586
79.924924	1326.028911	5.097011	-0.015844	2.078112
80.271739	1334.101528	5.102016	-0.015914	2.083637
80.512544	1342.190526	5.107021	-0.015964	2.089147
80.594599	1350.322974	5.112026	-0.015985	2.094656
80.992608	1358.379920	5.117030	-0.016065	2.100131
81.407963	1366.441536	5.122035	-0.016148	2.105597
81.455968	1374.622488	5.127040	-0.016162	2.111093
81.759351	1382.729107	5.132045	-0.016224	2.116549
81.894846	1390.797299	5.137050	-0.016255	2.121949
82.151451	1398.861455	5.142054	-0.016308	2.127345
82.221264	1406.969623	5.147059	-0.016326	2.132738
82.718022	1415.018922	5.152064	-0.016424	2.138120
83.117169	1423.070729	5.157069	-0.016504	2.143480
83.191788	1431.192321	5.162074	-0.016524	2.148841
83.579196	1439.308320	5.167078	-0.016601	2.154216
83.651956	1447.377614	5.172083	-0.016620	2.159516
83.725863	1455.478105	5.177088	-0.016640	2.164825
84.171929	1463.538130	5.182093	-0.016728	2.170128
84.312528	1471.637660	5.187098	-0.016760	2.175416
84.745316	1479.696275	5.192102	-0.016846	2.180691
84.766836	1487.790379	5.197107	-0.016855	2.185938
85.376490	1495.863460	5.202112	-0.016974	2.191214
85.880996	1503.918504	5.207117	-0.017074	2.196455
86.036384	1511.989768	5.212122	-0.017108	2.201662
86.424856	1520.065658	5.217126	-0.017186	2.206881
86.560357	1528.165840	5.222131	-0.017217	2.212081
86.818313	1536.265036	5.227136	-0.017270	2.217278
87.181809	1544.304126	5.232141	-0.017343	2.222435
87.442749	1552.400141	5.237146	-0.017397	2.227606
87.691592	1560.501839	5.242150	-0.017449	2.232768
87.858718	1568.552180	5.247155	-0.017486	2.237878
88.459530	1576.595628	5.252160	-0.017603	2.243011
88.914344	1584.654244	5.257165	-0.017693	2.248128
89.237685	1592.764288	5.262170	-0.017759	2.253254
89.565376	1600.849832	5.267174	-0.017826	2.258354
89.930587	1608.907979	5.272179	-0.017899	2.263428
90.218772	1616.998666	5.277184	-0.017958	2.268505
90.612500	1625.152283	5.282189	-0.018037	2.273618
90.915410	1633.195801	5.287194	-0.018099	2.278643
91.083722	1641.266817	5.292198	-0.018136	2.283663
91.186043	1649.333254	5.297203	-0.018160	2.288663
91.618988	1657.399478	5.302208	-0.018246	2.293681
92.020269	1665.447702	5.307213	-0.018326	2.298673
92.192669	1673.514637	5.312218	-0.018364	2.303647
92.470536	1681.594868	5.317222	-0.018421	2.308627
92.684418	1689.681343	5.322227	-0.018467	2.313595
93.277849	1697.700207	5.327232	-0.018583	2.318542
93.444108	1705.766477	5.332237	-0.018619	2.323473
93.605107	1713.855347	5.337242	-0.018654	2.328405
94.044571	1721.941353	5.342246	-0.018742	2.333349
94.179041	1730.012225	5.347251	-0.018772	2.338248
94.324217	1738.091691	5.352256	-0.018805	2.343143
94.646394	1746.146811	5.357261	-0.018870	2.348027
94.760608	1754.277200	5.362266	-0.018897	2.352929
95.053770	1762.338263	5.367270	-0.018957	2.357794
95.500060	1770.339723	5.372275	-0.019046	2.362626
96.133964	1778.370994	5.377280	-0.019169	2.367480
96.321271	1786.475095	5.382285	-0.019209	2.372332
96.692771	1794.517919	5.387290	-0.019284	2.377153
96.998308	1802.596956	5.392294	-0.019346	2.381980
96.988164	1810.676939	5.397299	-0.019350	2.386772
97.286240	1818.774955	5.402304	-0.019411	2.391590
97.621071	1826.828268	5.407309	-0.019479	2.396375
97.946347	1834.855458	5.412314	-0.019545	2.401133
98.110553	1842.942822	5.417318	-0.019581	2.405906
98.321565	1850.995972	5.422323	-0.019626	2.410652
98.693740	1859.074397	5.427328	-0.019700	2.415416
98.756282	1867.147316	5.432333	-0.019718	2.420143
99.139995	1875.177488	5.437338	-0.019795	2.424862
99.586866	1883.248997	5.442342	-0.019883	2.429599
99.721329	1891.400377	5.447347	-0.019914	2.434350
100.000311	1899.418436	5.452352	-0.019971	2.439026
100.445180	1907.427538	5.457357	-0.020059	2.443699
100.763921	1915.468847	5.462362	-0.020124	2.448373
101.299533	1923.534370	5.467366	-0.020229	2.453068
101.343319	1931.610705	5.472371	-0.020243	2.457724
101.733971	1939.655104	5.477376	-0.020321	2.462378
101.894916	1947.721848	5.482381	-0.020357	2.467019
101.878424	1955.815585	5.487386	-0.020359	2.471653
102.452490	1963.856334	5.492390	-0.020471	2.476292
102.519047	1971.908717	5.497395	-0.020489	2.480892
102.539913	1979.983677	5.502400	-0.020499	2.485492
103.001547	1988.024986	5.507405	-0.020590	2.490097
103.147122	1996.110015	5.512410	-0.020623	2.494696
103.571873	2004.137003	5.517414	-0.020707	2.499273
103.794989	2012.182626	5.522419	-0.020754	2.503838
104.086684	2020.260547	5.527424	-0.020814	2.508417
104.544728	2028.318978	5.532429	-0.020905	2.512989
104.671523	2036.391317	5.537434	-0.020934	2.517537
105.057715	2044.413322	5.542438	-0.021011	2.522067
105.201489	2052.481335	5.547443	-0.021044	2.526597
105.266800	2060.567816	5.552448	-0.021061	2.531123
105.668481	2068.614388	5.557453	-0.021141	2.535644
106.161787	2076.635572	5.562458	-0.021239	2.540148
106.596149	2084.678533	5.567462	-0.021325	2.544652
106.650369	2092.752552	5.572467	-0.021341	2.549139
106.974654	2100.830802	5.577472	-0.021406	2.553639
107.248210	2108.874026	5.582477	-0.021463	2.558108
107.286232	2116.923957	5.587482	-0.021475	2.562557
107.857500	2124.953973	5.592486	-0.021587	2.567024
107.960682	2133.028998	5.597491	-0.021612	2.571475
108.181064	2141.118398	5.602496	-0.021658	2.575935
108.382372	2149.174508	5.607501	-0.021701	2.580367
108.720579	2157.185749	5.612506	-0.021770	2.584777
109.105813	2165.245579	5.617510	-0.021847	2.589208
109.269859	2173.502350	5.622515	-0.021883	2.593724
109.763111	2181.482926	5.627520	-0.021980	2.598105
109.927337	2189.486153	5.632525	-0.022016	2.602468
110.087134	2197.486202	5.637530	-0.022052	2.606822
110.538443	2205.530062	5.642534	-0.022141	2.611211
110.863747	2213.545344	5.647539	-0.022207	2.615570
111.020784	2221.592751	5.652544	-0.022242	2.619927
111.357556	2229.617497	5.657549	-0.022310	2.624276
111.536105	2237.671552	5.662554	-0.022349	2.628624
111.916621	2245.746981	5.667558	-0.022425	2.632989
112.206452	2253.781122	5.672563	-0.022484	2.637319
112.617801	2261.812240	5.677568	-0.022567	2.641648
112.965733	2269.837112	5.682573	-0.022637	2.645962
113.196644	2277.886136	5.687578	-0.022685	2.650274
113.450635	2285.983987	5.692582	-0.022738	2.654607
113.597722	2294.018753	5.697587	-0.022771	2.658893
113.873879	2302.086112	5.702592	-0.022828	2.663197
114.111820	2310.132471	5.707597	-0.022878	2.667480
114.590707	2318.160238	5.712602	-0.022972	2.671762
114.775225	2326.275344	5.717606	-0.023012	2.676065
114.781687	2334.296773	5.722611	-0.023019	2.680299
115.213351	2342.283570	5.727616	-0.023104	2.684536
115.486574	2350.354650	5.732621	-0.023161	2.688800
115.485490	2358.428400	5.737626	-0.023166	2.693042
115.838199	2366.480599	5.742630	-0.023237	2.697288
116.075017	2374.499979	5.747635	-0.023287	2.701503
116.599285	2382.514835	5.752640	-0.023390	2.705726
116.767239	2390.587045	5.757645	-0.023427	2.709951
117.010873	2398.653908	5.762650	-0.023477	2.714171
117.268219	2406.695214	5.767654	-0.023531	2.718372
117.412692	2414.716886	5.772659	-0.023563	2.722549
117.808375	2422.755371	5.777664	-0.023642	2.726744
117.914132	2430.828286	5.782669	-0.023667	2.730933
118.084392	2438.892715	5.787674	-0.023705	2.735114
118.365247	2446.923813	5.792678	-0.023762	2.739279
118.789184	2454.932799	5.797683	-0.023847	2.743435
119.212975	2462.983324	5.802688	-0.023931	2.747606
119.423652	2471.090919	5.807693	-0.023976	2.751786
119.632367	2479.178942	5.812698	-0.024020	2.755950
120.050847	2487.190047	5.817702	-0.024104	2.760081
119.838031	2495.225825	5.822707	-0.024069	2.764181
120.336969	2503.239553	5.827712	-0.024168	2.768306
120.500571	2511.312710	5.832717	-0.024204	2.772434
120.581835	2519.354877	5.837722	-0.024224	2.776536
120.916021	2527.396088	5.842726	-0.024292	2.780647
121.134042	2535.385413	5.847731	-0.024338	2.784718
121.542887	2543.432147	5.852736	-0.024420	2.788823
121.723001	2551.518125	5.857741	-0.024459	2.792929
121.924981	2559.543149	5.862746	-0.024502	2.796999
122.410436	2567.562061	5.867750	-0.024597	2.801077
122.335710	2575.609259	5.872755	-0.024589	2.805130
122.761600	2583.632722	5.877760	-0.024674	2.809195
123.210619	2591.683413	5.882765	-0.024763	2.813268
123.387472	2599.724385	5.887770	-0.024801	2.817315
123.530520	2607.797728	5.892774	-0.024833	2.821371
123.786012	2615.818730	5.897779	-0.024886	2.825401
124.075178	2623.863112	5.902784	-0.024946	2.829439
124.253501	2631.966846	5.907789	-0.024984	2.833494
124.397665	2639.979628	5.912794	-0.025017	2.837496
124.690825	2648.013239	5.917798	-0.025077	2.841511
124.647831	2656.055036	5.922803	-0.025074	2.845506
124.969128	2664.062451	5.927808	-0.025139	2.849498
125.247894	2672.132735	5.932813	-0.025197	2.853514
125.504038	2680.147035	5.937818	-0.025250	2.857494
125.869666	2688.198250	5.942822	-0.025323	2.861494
126.033859	2696.225992	5.947827	-0.025359	2.865465
126.233195	2704.261656	5.952832	-0.025402	2.869437
126.398082	2712.353058	5.957837	-0.025438	2.873428
126.430571	2720.378454	5.962842	-0.025450	2.877374
126.944002	2728.383447	5.967846	-0.025551	2.881332
126.969891	2736.434339	5.972851	-0.025561	2.885279
127.251170	2744.471679	5.977856	-0.025619	2.889228
127.545407	2752.541748	5.982861	-0.025679	2.893189
127.659015	2760.579715	5.987866	-0.025706	2.897119
127.779853	2768.643888	5.992870	-0.025734	2.901056
128.066686	2776.621160	5.997875	-0.025793	2.904955
128.572728	2784.656459	6.002880	-0.025892	2.908888
129.023596	2792.773990	6.007885	-0.025982	2.912853
129.240111	2800.804229	6.012890	-0.026027	2.916758
129.740188	2808.821975	6.017894	-0.026126	2.920666
129.718389	2816.807762	6.022899	-0.026127	2.924526
130.162322	2824.863150	6.027904	-0.026216	2.928439
130.580110	2832.896135	6.032909	-0.026299	2.932335
130.506790	2840.987062	6.037914	-0.026291	2.936228
130.763283	2848.980065	6.042918	-0.026344	2.940085
131.082852	2856.987268	6.047923	-0.026409	2.943948
131.213490	2865.062116	6.052928	-0.026439	2.947828
131.484560	2873.108357	6.057933	-0.026494	2.951696
131.846519	2881.141124	6.062938	-0.026567	2.955558
132.141535	2889.172197	6.067942	-0.026628	2.959410
132.317467	2897.188083	6.072947	-0.026666	2.963244
132.376939	2905.247284	6.077952	-0.026682	2.967087
132.725575	2913.291879	6.082957	-0.026753	2.970934
132.848363	2921.352859	6.087962	-0.026781	2.974771
132.899428	2929.385254	6.092966	-0.026796	2.978587
133.124408	2937.392305	6.097971	-0.026843	2.982394
133.399351	2945.454542	6.102976	-0.026900	2.986225
133.401104	2953.504117	6.107981	-0.026906	2.990031
133.627726	2961.554664	6.112986	-0.026954	2.993844
133.897192	2969.579936	6.117990	-0.027009	2.997643
134.110011	2977.581066	6.122995	-0.027054	3.001422
134.269164	2985.592747	6.128000	-0.027089	3.005199
134.578153	2993.624756	6.133005	-0.027152	3.008989
134.630436	3001.683380	6.138010	-0.027168	3.012773
134.665845	3009.765273	6.143014	-0.027180	3.016562
134.947023	3017.752873	6.148019	-0.027237	3.020315
135.452706	3025.729775	6.153024	-0.027337	3.024069
135.716186	3033.784941	6.158029	-0.027391	3.027843
135.994597	3041.821950	6.163034	-0.027449	3.031604
136.419940	3049.908159	6.168038	-0.027533	3.035391
136.655829	3057.912187	6.173043	-0.027583	3.039125
136.731933	3065.968953	6.178048	-0.027602	3.042872
137.135751	3074.007225	6.183053	-0.027683	3.046621
137.188240	3082.018370	6.188058	-0.027698	3.050336
137.506870	3090.084138	6.193062	-0.027763	3.054085
137.804621	3098.089829	6.198067	-0.027824	3.057800
138.084257	3106.132308	6.203072	-0.027882	3.061527
138.359295	3114.175049	6.208077	-0.027938	3.065249
138.507160	3122.178308	6.213082	-0.027971	3.068942
138.907158	3130.301396	6.218086	-0.028051	3.072698
139.082962	3138.364986	6.223091	-0.028089	3.076411
139.016772	3146.349998	6.228096	-0.028082	3.080073
139.534937	3154.338409	6.233101	-0.028184	3.083759
139.647426	3162.344258	6.238106	-0.028211	3.087429
139.919080	3170.395546	6.243110	-0.028267	3.091124
140.251633	3178.424485	6.248115	-0.028334	3.094806
140.501464	3186.449572	6.253120	-0.028386	3.098478
140.748947	3194.498262	6.258125	-0.028438	3.102157
140.854632	3202.516620	6.263130	-0.028463	3.105811
141.215238	3210.558163	6.268134	-0.028535	3.109483
141.340122	3218.630175	6.273139	-0.028564	3.113153
141.555634	3226.662805	6.278144	-0.028610	3.116806
142.018714	3234.663120	6.283149	-0.028701	3.120450
142.179966	3242.644287	6.288154	-0.028737	3.124068
142.488392	3250.713544	6.293158	-0.028800	3.127729
142.707969	3258.759673	6.298163	-0.028846	3.131370
142.976231	3266.803556	6.303168	-0.028901	3.135009
143.271505	3274.832069	6.308173	-0.028962	3.138637
143.471319	3282.850931	6.313178	-0.029005	3.142253
143.698358	3290.913321	6.318182	-0.029052	3.145885
143.860586	3298.933713	6.323187	-0.029088	3.149491
144.014814	3306.997621	6.328192	-0.029122	3.153112
144.360936	3315.008224	6.333197	-0.029192	3.156714
144.715961	3323.016114	6.338202	-0.029264	3.160310
144.827741	3331.048533	6.343206	-0.029290	3.163903
144.804146	3339.098360	6.348211	-0.029291	3.167494
145.147384	3347.116942	6.353216	-0.029360	3.171082
145.479117	3355.185194	6.358221	-0.029428	3.174688
145.552380	3363.178087	6.363226	-0.029447	3.178245
145.938529	3371.219539	6.368230	-0.029524	3.181833
145.977886	3379.228892	6.373235	-0.029537	3.185388
146.306718	3387.268856	6.378240	-0.029603	3.188965
146.429696	3395.324272	6.383245	-0.029632	3.192536
146.628074	3403.371699	6.388250	-0.029674	3.196103
146.862007	3411.369670	6.393254	-0.029723	3.199645
146.946398	3419.386575	6.398259	-0.029744	3.203185
147.216731	3427.422429	6.403264	-0.029800	3.206738
147.609583	3435.464978	6.408269	-0.029879	3.210294
147.701004	3443.509565	6.413274	-0.029901	3.213835
147.950932	3451.559533	6.418278	-0.029953	3.217381
148.319253	3459.571076	6.423283	-0.030027	3.220911
148.234652	3467.569201	6.428288	-0.030017	3.224413
148.503158	3475.625720	6.433293	-0.030072	3.227951
149.006964	3483.652103	6.438298	-0.030172	3.231481
149.122573	3491.750866	6.443302	-0.030199	3.235024
149.339111	3499.695977	6.448307	-0.030244	3.238499
149.606267	3507.718859	6.453312	-0.030300	3.242007
150.022376	3515.744668	6.458317	-0.030382	3.245518
150.062317	3523.763140	6.463322	-0.030395	3.249006
150.266716	3531.841965	6.468326	-0.030439	3.252524
150.590874	3539.877596	6.473331	-0.030505	3.256024
150.714870	3547.851784	6.478336	-0.030533	3.259486
150.898868	3555.913418	6.483341	-0.030573	3.262984
151.103015	3563.929243	6.488346	-0.030616	3.266460
151.467692	3571.971599	6.493350	-0.030690	3.269949
151.419770	3580.044369	6.498355	-0.030686	3.273432
151.578894	3588.056925	6.503360	-0.030721	3.276893
151.945232	3596.051277	6.508365	-0.030795	3.280350
152.115836	3604.062514	6.513370	-0.030832	3.283804
152.535393	3612.080156	6.518374	-0.030916	3.287266
152.680293	3620.137017	6.523379	-0.030948	3.290731
152.986393	3628.174852	6.528384	-0.031011	3.294190
153.040403	3636.241709	6.533389	-0.031026	3.297648
153.345436	3644.232571	6.538394	-0.031088	3.301080
153.874426	3652.227251	6.543398	-0.031192	3.304518
153.994658	3660.269860	6.548403	-0.031220	3.307958
154.074848	3668.353018	6.553408	-0.031241	3.311410
154.355120	3676.401258	6.558413	-0.031298	3.314850
154.372291	3684.413056	6.563418	-0.031307	3.318262
154.513421	3692.420699	6.568422	-0.031339	3.321673
154.850296	3700.408375	6.573427	-0.031407	3.325080
155.170640	3708.441189	6.578432	-0.031472	3.328501
155.166912	3716.518224	6.583437	-0.031477	3.331926
155.488038	3724.529420	6.588442	-0.031542	3.335331
155.841062	3732.532890	6.593446	-0.031613	3.338730
155.962571	3740.581124	6.598451	-0.031641	3.342137
156.062136	3748.581843	6.603456	-0.031665	3.345519
156.661093	3756.623665	6.608461	-0.031782	3.348933
156.590939	3764.693353	6.613466	-0.031775	3.352331
156.677093	3772.760674	6.618470	-0.031796	3.355730
156.912617	3780.752791	6.623475	-0.031845	3.359100
157.437527	3788.737842	6.628480	-0.031949	3.362473
157.635203	3796.780075	6.633485	-0.031991	3.365856
158.012461	3804.764471	6.638490	-0.032066	3.369217
158.355296	3812.823356	6.643494	-0.032136	3.372605
158.396996	3820.904222	6.648499	-0.032149	3.375987
158.405417	3828.878728	6.653504	-0.032156	3.379321
158.654261	3836.927501	6.658509	-0.032208	3.382691
158.939208	3844.957413	6.663514	-0.032266	3.386051
158.965910	3853.004498	6.668518	-0.032277	3.389405
159.138839	3861.084774	6.673523	-0.032314	3.392776
159.675378	3869.100570	6.678528	-0.032420	3.396128
159.875014	3877.073102	6.683533	-0.032462	3.399448
160.165439	3885.038412	6.688538	-0.032522	3.402764
160.344472	3893.126381	6.693542	-0.032561	3.406125
160.471505	3901.119694	6.698547	-0.032590	3.409440
160.613888	3909.147504	6.703552	-0.032622	3.412768
161.002420	3917.204382	6.708557	-0.032700	3.416113
161.200018	3925.160355	6.713562	-0.032742	3.419406
161.367983	3933.214344	6.718566	-0.032778	3.422735
161.525871	3941.273302	6.723571	-0.032813	3.426063
161.685809	3949.270236	6.728576	-0.032849	3.429362
162.280874	3957.334981	6.733581	-0.032965	3.432700
162.547357	3965.355673	6.738586	-0.033020	3.436006
162.675443	3973.355185	6.743590	-0.033049	3.439295
163.012527	3981.376650	6.748595	-0.033117	3.442597
162.984293	3989.404360	6.753600	-0.033118	3.445887
163.153538	3997.459612	6.758605	-0.033155	3.449191
163.577707	4005.480722	6.763610	-0.033239	3.452486
163.908913	4013.542408	6.768614	-0.033306	3.455792
163.954256	4021.525534	6.773619	-0.033320	3.459053
164.091373	4029.545625	6.778624	-0.033351	3.462328
164.375522	4037.571596	6.783629	-0.033409	3.465608
164.370142	4045.645272	6.788634	-0.033414	3.468895
164.675594	4053.677315	6.793638	-0.033476	3.472172
165.096613	4061.700242	6.798643	-0.033560	3.475446
165.056192	4069.684360	6.803648	-0.033558	3.478686
165.309811	4077.716616	6.808653	-0.033611	3.481952
165.575346	4085.708578	6.813658	-0.033665	3.485199
165.903039	4093.714814	6.818662	-0.033732	3.488450
166.067519	4101.787807	6.823667	-0.033768	3.491721
166.277138	4109.812359	6.828672	-0.033812	3.494970
166.423172	4117.867236	6.833677	-0.033845	3.498226
166.287140	4125.866441	6.838682	-0.033825	3.501448
166.552684	4133.863508	6.843686	-0.033880	3.504678
166.878312	4141.920849	6.848691	-0.033946	3.507932
167.086705	4149.947506	6.853696	-0.033990	3.511167
167.338353	4157.977561	6.858701	-0.034043	3.514401
167.783435	4165.966823	6.863706	-0.034131	3.517622
168.162719	4174.016167	6.868710	-0.034207	3.520862
168.285638	4181.983567	6.873715	-0.034235	3.524059
168.385564	4190.056763	6.878720	-0.034259	3.527294
168.913715	4198.077536	6.883725	-0.034363	3.530518
168.783225	4206.140202	6.888730	-0.034344	3.533736
168.994579	4214.178052	6.893734	-0.034389	3.536951
169.273413	4222.191604	6.898739	-0.034447	3.540156
169.151868	4230.205841	6.903744	-0.034429	3.543346
169.422440	4238.255877	6.908749	-0.034485	3.546559
169.548645	4246.242489	6.913754	-0.034514	3.549740
169.647583	4254.392406	6.918758	-0.034538	3.552981
169.732825	4262.443070	6.923763	-0.034559	3.556181
170.199229	4270.324699	6.928768	-0.034652	3.559321
170.373530	4278.346260	6.933773	-0.034690	3.562505
170.485253	4286.357623	6.938778	-0.034716	3.565681
170.762134	4294.375068	6.943782	-0.034773	3.568861
171.258517	4302.419226	6.948787	-0.034871	3.572055
171.129219	4310.466852	6.953792	-0.034852	3.575230
171.287100	4318.475254	6.958797	-0.034887	3.578394
171.563574	4326.493270	6.963802	-0.034944	3.581563
171.903576	4334.467114	6.968806	-0.035013	3.584713
172.069117	4342.521107	6.973811	-0.035049	3.587888
172.238950	4350.554200	6.978816	-0.035086	3.591051
172.538444	4358.585904	6.983821	-0.035147	3.594214
172.552586	4366.624662	6.988826	-0.035155	3.597370
172.826066	4374.607282	6.993830	-0.035212	3.600508
173.289217	4382.613722	6.998835	-0.035303	3.603657
173.035807	4390.656966	7.003840	-0.035262	3.606799
173.342999	4398.700767	7.008845	-0.035324	3.609953
173.794146	4406.708764	7.013850	-0.035414	3.613095
174.180803	4414.743706	7.018854	-0.035491	3.616243
174.195033	4422.742449	7.023859	-0.035499	3.619363
174.595251	4430.724151	7.028864	-0.035579	3.622485
174.978759	4438.790300	7.033869	-0.035656	3.625636
175.002894	4446.837417	7.038874	-0.035666	3.628767
175.077586	4454.912081	7.043878	-0.035685	3.631908
175.268499	4462.947889	7.048883	-0.035726	3.635034
175.421510	4470.932970	7.053888	-0.035760	3.638137
175.841977	4478.949131	7.058893	-0.035844	3.641256
176.154237	4486.918550	7.063898	-0.035908	3.644352
176.397033	4494.973915	7.068902	-0.035958	3.647476
176.460184	4503.000170	7.073907	-0.035975	3.650581
176.611259	4511.066889	7.078912	-0.036009	3.653702
176.765604	4519.127413	7.083917	-0.036043	3.656818
176.775550	4527.081628	7.088922	-0.036050	3.659886
177.053416	4535.094862	7.093926	-0.036108	3.662981
177.197624	4543.154871	7.098931	-0.036140	3.666089
177.501168	4551.144473	7.103936	-0.036202	3.669171
177.701726	4559.231551	7.108941	-0.036245	3.672284
177.958280	4567.244580	7.113946	-0.036298	3.675369
178.175746	4575.216614	7.118950	-0.036344	3.678433
178.308081	4583.248322	7.123955	-0.036374	3.681516
178.601224	4591.223146	7.128960	-0.036434	3.684579
178.941628	4599.295446	7.133965	-0.036503	3.687678
178.900534	4607.337025	7.138970	-0.036501	3.690752
179.103077	4615.377419	7.143974	-0.036544	3.693830
179.247735	4623.394881	7.148979	-0.036576	3.696895
179.278515	4631.365944	7.153984	-0.036587	3.699937
179.624640	4639.394277	7.158989	-0.036657	3.703006
179.836438	4647.425058	7.163994	-0.036702	3.706069
180.119805	4655.430855	7.168998	-0.036760	3.709123
180.216118	4663.540918	7.174003	-0.036784	3.712209
180.529922	4671.589487	7.179008	-0.036848	3.715275
180.888562	4679.597535	7.184013	-0.036920	3.718323
180.889402	4687.578451	7.189018	-0.036925	3.721350
181.070464	4695.505725	7.194022	-0.036965	3.724359
181.237410	4703.566591	7.199027	-0.037001	3.727416
181.543964	4711.568324	7.204032	-0.037064	3.730450
181.696823	4719.641807	7.209037	-0.037098	3.733506
181.842953	4727.650469	7.214042	-0.037130	3.736535
182.179904	4735.650374	7.219046	-0.037198	3.739562
182.247617	4743.682930	7.224051	-0.037216	3.742593
182.297192	4751.680898	7.229056	-0.037231	3.745608
182.754971	4759.713792	7.234061	-0.037322	3.748643
182.809204	4767.769371	7.239066	-0.037337	3.751675
182.909061	4775.813714	7.244070	-0.037361	3.754701
183.323937	4783.810203	7.249075	-0.037444	3.757714
183.523957	4791.826536	7.254080	-0.037487	3.760727
183.904282	4799.821663	7.259085	-0.037563	3.763734
183.898663	4807.877826	7.264090	-0.037567	3.766752
184.157789	4815.893433	7.269094	-0.037621	3.769759
184.684986	4823.935993	7.274099	-0.037725	3.772780
184.791036	4831.984868	7.279104	-0.037750	3.775791
185.128062	4839.974414	7.284109	-0.037818	3.778782
185.202567	4848.016390	7.289114	-0.037837	3.781785
185.482820	4855.998836	7.294118	-0.037895	3.784768
185.682290	4864.063798	7.299123	-0.037938	3.787777
186.082868	4872.051122	7.304128	-0.038018	3.790759
186.408398	4880.132503	7.309133	-0.038084	3.793773
186.353104	4888.163202	7.314138	-0.038079	3.796756
186.690802	4896.118120	7.319142	-0.038147	3.799718
186.995597	4904.154558	7.324147	-0.038209	3.802707
187.025733	4912.125978	7.329152	-0.038220	3.805664
187.273638	4920.170118	7.334157	-0.038272	3.808650
187.631800	4928.202449	7.339162	-0.038344	3.811631
187.719331	4936.213053	7.344166	-0.038366	3.814597
187.841454	4944.250746	7.349171	-0.038394	3.817570
188.120339	4952.227374	7.354176	-0.038452	3.820522
188.365480	4960.256246	7.359181	-0.038503	3.823491
188.409568	4968.264885	7.364186	-0.038516	3.826445
188.651052	4976.313385	7.369190	-0.038567	3.829416
188.850755	4984.379109	7.374195	-0.038609	3.832390
188.894555	4992.353926	7.379200	-0.038623	3.835325
189.283053	5000.394397	7.384205	-0.038701	3.838289
189.266004	5008.411396	7.389210	-0.038703	3.841234
189.318241	5016.393219	7.394214	-0.038718	3.844165
189.624097	5024.459788	7.399219	-0.038781	3.847130
189.796003	5032.461789	7.404224	-0.038818	3.850066
190.025943	5040.537540	7.409229	-0.038866	3.853028
190.038437	5048.549719	7.414234	-0.038874	3.855960
190.390406	5056.547570	7.419238	-0.038945	3.858892
190.739673	5064.550101	7.424243	-0.039016	3.861823
190.804266	5072.557356	7.429248	-0.039033	3.864747
190.960874	5080.626474	7.434253	-0.039068	3.867694
191.314781	5088.631971	7.439258	-0.039139	3.870620
191.365936	5096.923325	7.444262	-0.039154	3.873641
191.442845	5104.888567	7.449267	-0.039174	3.876541
191.635121	5112.766876	7.454272	-0.039215	3.879411
192.052338	5120.775685	7.459277	-0.039298	3.882329
192.064572	5128.746121	7.464282	-0.039306	3.885224
192.447915	5136.750958	7.469286	-0.039383	3.888136
192.609239	5144.790108	7.474291	-0.039418	3.891054
192.521249	5152.843371	7.479296	-0.039407	3.893971
192.726575	5160.874261	7.484301	-0.039451	3.896882
192.996120	5168.806020	7.489306	-0.039506	3.899757
193.232649	5176.862970	7.494310	-0.039556	3.902674
193.359681	5184.867781	7.499315	-0.039585	3.905568
193.468969	5192.844903	7.504320	-0.039611	3.908450
193.589737	5200.958982	7.509325	-0.039639	3.911379
193.616592	5208.958396	7.514330	-0.039649	3.914263
194.011423	5216.993417	7.519334	-0.039728	3.917164
194.239255	5224.952853	7.524339	-0.039776	3.920033
194.354075	5232.947423	7.529344	-0.039803	3.922910
194.645390	5241.021534	7.534349	-0.039863	3.925817
194.764120	5249.018286	7.539354	-0.039890	3.928691
194.791301	5257.048187	7.544358	-0.039901	3.931573
194.927935	5265.108999	7.549363	-0.039932	3.934466
195.051978	5273.077071	7.554368	-0.039960	3.937323
195.204466	5281.125465	7.559373	-0.039994	3.940207
195.365970	5289.113041	7.564378	-0.040029	3.943068
195.741026	5297.120418	7.569382	-0.040105	3.945937
195.922023	5305.159936	7.574387	-0.040144	3.948813
196.099968	5313.154808	7.579392	-0.040182	3.951670
196.407696	5321.255156	7.584397	-0.040245	3.954565
196.434693	5329.266569	7.589402	-0.040256	3.957421
196.709468	5337.238490	7.594406	-0.040312	3.960266
196.845482	5345.236988	7.599411	-0.040343	3.963115
197.149657	5353.244656	7.604416	-0.040405	3.965969
197.559859	5361.262827	7.609421	-0.040487	3.968826
197.535192	5369.312045	7.614426	-0.040488	3.971684
197.830594	5377.344854	7.619430	-0.040548	3.974540
198.070327	5385.365947	7.624435	-0.040598	3.977389
198.159403	5393.350631	7.629440	-0.040620	3.980220
198.407538	5401.396214	7.634445	-0.040672	3.983074
198.554825	5409.403842	7.639450	-0.040705	3.985910
198.888456	5417.401531	7.644454	-0.040772	3.988744
198.976331	5425.508324	7.649459	-0.040794	3.991610
199.378834	5433.499499	7.654464	-0.040875	3.994439
199.670529	5441.532570	7.659469	-0.040934	3.997278
199.774461	5449.527796	7.664474	-0.040959	4.000099
199.866141	5457.550546	7.669478	-0.040982	4.002928
200.255812	5465.581500	7.674483	-0.041060	4.005762
200.204973	5473.574253	7.679488	-0.041056	4.008574
200.469911	5481.665911	7.684493	-0.041110	4.011423
200.660323	5489.653890	7.689498	-0.041151	4.014233
200.847443	5497.714409	7.694502	-0.041192	4.017066
200.967552	5505.706234	7.699507	-0.041219	4.019872
201.136652	5513.682838	7.704512	-0.041256	4.022672
201.385543	5521.722186	7.709517	-0.041308	4.025492
201.502010	5529.773962	7.714522	-0.041335	4.028314
201.772168	5537.777449	7.719526	-0.041391	4.031118
202.068733	5545.931082	7.724531	-0.041452	4.033973
202.404842	5553.886910	7.729536	-0.041520	4.036758
202.406949	5561.850186	7.734541	-0.041526	4.039539
202.431625	5569.832315	7.739546	-0.041536	4.042324
202.586460	5577.812643	7.744550	-0.041570	4.045109
202.582284	5585.886837	7.749555	-0.041575	4.047922
202.817615	5593.885706	7.754560	-0.041624	4.050711
203.178524	5601.919036	7.759565	-0.041696	4.053511
203.379348	5609.963863	7.764570	-0.041739	4.056311
203.212749	5617.938822	7.769574	-0.041714	4.059080
203.926319	5625.993405	7.774579	-0.041852	4.061887
203.827215	5633.913593	7.779584	-0.041839	4.064634
204.049584	5642.007877	7.784589	-0.041886	4.067443
204.183278	5650.010527	7.789594	-0.041916	4.070218
204.481110	5658.049022	7.794598	-0.041977	4.073006
204.604424	5666.105617	7.799603	-0.042006	4.075795
204.614766	5674.051304	7.804608	-0.042013	4.078543
204.992684	5682.068101	7.809613	-0.042089	4.081319
205.138779	5690.060854	7.814618	-0.042121	4.084081
205.344640	5698.111023	7.819622	-0.042165	4.086861
205.445243	5706.129254	7.824627	-0.042189	4.089628
205.690392	5714.130079	7.829632	-0.042240	4.092388
205.751747	5722.231553	7.834637	-0.042257	4.095179
205.883845	5730.226034	7.839642	-0.042287	4.097932
206.117942	5738.195678	7.844646	-0.042336	4.100676
206.430844	5746.194998	7.849651	-0.042400	4.103429
206.419117	5754.225880	7.854656	-0.042403	4.106187
206.728306	5762.260877	7.859661	-0.042466	4.108949
206.884982	5770.321757	7.864666	-0.042501	4.111716
206.960562	5778.378436	7.869670	-0.042520	4.114478
207.120872	5786.389069	7.874675	-0.042556	4.117224
207.244105	5794.349022	7.879680	-0.042584	4.119950
207.299000	5802.372534	7.884685	-0.042600	4.122695
207.530576	5810.373896	7.889690	-0.042648	4.125433
207.725406	5818.371968	7.894694	-0.042690	4.128168
207.952964	5826.458407	7.899699	-0.042738	4.130931
208.001365	5834.473553	7.904704	-0.042752	4.133666
208.248919	5842.535401	7.909709	-0.042804	4.136417
208.465658	5850.471828	7.914714	-0.042850	4.139124
208.556462	5858.535457	7.919718	-0.042872	4.141870
209.088657	5866.523641	7.924723	-0.042977	4.144594
209.144842	5874.582798	7.929728	-0.042992	4.147335
209.470839	5882.598319	7.934733	-0.043059	4.150063
209.635439	5890.633170	7.939738	-0.043095	4.152793
209.908336	5898.640172	7.944742	-0.043151	4.155513
210.100113	5906.635080	7.949747	-0.043192	4.158226
210.041440	5914.642973	7.954752	-0.043187	4.160939
210.189300	5922.610294	7.959757	-0.043220	4.163639
210.471791	5930.713013	7.964762	-0.043278	4.166385
210.647286	5938.681684	7.969766	-0.043316	4.169082
210.941547	5946.737543	7.974771	-0.043376	4.171808
211.057422	5954.711365	7.979776	-0.043403	4.174503
211.236435	5962.790074	7.984781	-0.043442	4.177232
211.455998	5970.772822	7.989786	-0.043488	4.179927
211.461434	5978.803041	7.994790	-0.043495	4.182634
211.664778	5986.794018	7.999795	-0.043538	4.185328
211.901968	5994.792849	8.004800	-0.043587	4.188024
212.251606	6002.873148	8.009805	-0.043658	4.190746
212.302998	6010.976754	8.014810	-0.043673	4.193471
212.490934	6018.998599	8.019814	-0.043714	4.196169
212.796945	6026.923372	8.024819	-0.043776	4.198833
213.034701	6034.902919	8.029824	-0.043826	4.201513
213.181033	6042.880275	8.034829	-0.043858	4.204190
213.180477	6050.945615	8.039834	-0.043864	4.206893
213.489904	6058.912417	8.044838	-0.043927	4.209565
213.984988	6066.986961	8.049843	-0.044024	4.212272
213.867948	6074.986574	8.054848	-0.044008	4.214947
214.070371	6083.023609	8.059853	-0.044051	4.217636
214.258919	6090.990557	8.064858	-0.044092	4.220299
214.404770	6099.045281	8.069862	-0.044124	4.222989
214.468103	6107.045877	8.074867	-0.044141	4.225659
214.787729	6115.047763	8.079872	-0.044206	4.228331
215.130855	6123.086962	8.084877	-0.044276	4.231013
215.086929	6131.155793	8.089882	-0.044273	4.233699
215.256399	6139.184163	8.094886	-0.044310	4.236373
215.352095	6147.137162	8.099891	-0.044333	4.239018
215.506536	6155.170552	8.104896	-0.044368	4.241690
215.687353	6163.145337	8.109901	-0.044407	4.244341
215.870831	6171.206023	8.114906	-0.044446	4.247018
215.816790	6179.230494	8.119910	-0.044442	4.249679
215.956820	6187.286632	8.124915	-0.044473	4.252352
216.180851	6195.265471	8.129920	-0.044520	4.254997
216.250424	6203.316787	8.134925	-0.044539	4.257664
216.313750	6211.281810	8.139930	-0.044556	4.260300
216.333741	6219.315295	8.144934	-0.044565	4.262957
216.643321	6227.335671	8.149939	-0.044628	4.265610
216.803549	6235.332044	8.154944	-0.044663	4.268253
216.850408	6243.383739	8.159949	-0.044678	4.270911
217.268619	6251.467689	8.164954	-0.044761	4.273581
217.390546	6259.464146	8.169958	-0.044789	4.276218
217.612499	6267.467759	8.174963	-0.044836	4.278857
217.865191	6275.461397	8.179968	-0.044888	4.281491
218.195127	6283.414449	8.184973	-0.044955	4.284110
218.211127	6291.487729	8.189978	-0.044964	4.286765
218.300001	6299.458727	8.194982	-0.044986	4.289386
218.424955	6307.585888	8.199987	-0.045014	4.292056
218.492036	6315.548328	8.204992	-0.045032	4.294670
218.903803	6323.602450	8.209997	-0.045114	4.297315
219.175079	6331.578419	8.215002	-0.045170	4.299932
219.181007	6339.587659	8.220006	-0.045177	4.302556
219.275813	6347.600635	8.225011	-0.045200	4.305181
219.461984	6355.632614	8.230016	-0.045240	4.307810
219.665132	6363.679692	8.235021	-0.045283	4.310443
219.796299	6371.685673	8.240026	-0.045313	4.313061
219.883826	6379.742524	8.245030	-0.045335	4.315693
219.942346	6387.733243	8.250035	-0.045351	4.318302
220.116822	6395.723328	8.255040	-0.045389	4.320910
220.360617	6403.729215	8.260045	-0.045440	4.323521
220.387715	6411.760207	8.265050	-0.045451	4.326138
220.725978	6419.722081	8.270054	-0.045519	4.328733
220.997457	6427.812214	8.275059	-0.045575	4.331368
221.042871	6435.782656	8.280064	-0.045589	4.333960
221.098561	6443.833581	8.285069	-0.045605	4.336578
221.341890	6451.815224	8.290074	-0.045655	4.339172
221.436994	6459.832772	8.295078	-0.045679	4.341775
221.951666	6467.797322	8.300083	-0.045780	4.344363
221.981354	6475.851999	8.305088	-0.045791	4.346975
222.131167	6483.905222	8.310093	-0.045824	4.349585
222.334649	6491.969013	8.315098	-0.045868	4.352198
222.452301	6500.041396	8.320102	-0.045895	4.354812
222.757014	6508.037718	8.325107	-0.045957	4.357400
222.989449	6515.928288	8.330112	-0.046006	4.359952
223.136650	6523.986674	8.335117	-0.046039	4.362557
223.192157	6531.954994	8.340122	-0.046054	4.365130
223.199031	6539.956075	8.345126	-0.046061	4.367712
223.608393	6548.008503	8.350131	-0.046143	4.370311
224.051762	6556.008092	8.355136	-0.046231	4.372892
224.040081	6564.078240	8.360141	-0.046234	4.375491
224.080435	6572.109549	8.365146	-0.046247	4.378077
224.259727	6580.041185	8.370150	-0.046286	4.380630
224.426422	6588.113729	8.375155	-0.046322	4.383227
224.444348	6596.108257	8.380160	-0.046331	4.385796
224.701710	6604.137313	8.385165	-0.046384	4.388376
224.776607	6612.164647	8.390170	-0.046404	4.390953
225.138537	6620.198616	8.395174	-0.046477	4.393532
225.215091	6628.276403	8.400179	-0.046496	4.396122
225.233409	6636.196220	8.405184	-0.046505	4.398659
225.500124	6644.217928	8.410189	-0.046560	4.401229
225.697025	6652.208503	8.415194	-0.046602	4.403787
225.734813	6660.254236	8.420198	-0.046615	4.406361
225.969837	6668.258547	8.425203	-0.046664	4.408921
226.145867	6676.276366	8.430208	-0.046702	4.411483
226.206101	6684.338883	8.435213	-0.046719	4.414057
226.299403	6692.399757	8.440218	-0.046742	4.416630
226.616352	6700.358160	8.445222	-0.046806	4.419169
226.892080	6708.439480	8.450227	-0.046863	4.421746
227.021326	6716.358192	8.455232	-0.046893	4.424269
227.318005	6724.434027	8.460237	-0.046953	4.426841
227.309075	6732.421929	8.465242	-0.046957	4.429383
227.476298	6740.470838	8.470246	-0.046994	4.431943
227.601933	6748.560440	8.475251	-0.047023	4.434514
227.640185	6756.488847	8.480256	-0.047035	4.437032
228.086469	6764.456535	8.485261	-0.047124	4.439563
228.315290	6772.503752	8.490266	-0.047172	4.442117
228.633400	6780.437297	8.495270	-0.047236	4.444634
228.772170	6788.554238	8.500275	-0.047268	4.447206
228.990732	6796.516144	8.505280	-0.047314	4.449728
229.229143	6804.592921	8.510285	-0.047364	4.452286
229.347698	6812.624606	8.515290	-0.047391	4.454827
229.503218	6820.618987	8.520294	-0.047425	4.457354
229.633656	6828.616303	8.525299	-0.047455	4.459882
229.652789	6836.655146	8.530304	-0.047464	4.462420
229.958495	6844.644752	8.535309	-0.047527	4.464943
230.001767	6852.680649	8.540314	-0.047540	4.467478
230.047011	6860.669597	8.545318	-0.047554	4.469996
230.289777	6868.752068	8.550323	-0.047605	4.472543
230.583297	6876.727613	8.555328	-0.047665	4.475056
230.697423	6884.782137	8.560333	-0.047691	4.477591
230.676848	6892.751353	8.565338	-0.047693	4.480097
230.892700	6900.761325	8.570343	-0.047739	4.482616
231.028430	6908.758817	8.575347	-0.047769	4.485128
230.941859	6916.795898	8.580352	-0.047759	4.487652
231.172509	6924.784612	8.585357	-0.047807	4.490159
231.489975	6932.864683	8.590362	-0.047872	4.492694
231.639588	6940.870328	8.595367	-0.047905	4.495204
231.892478	6948.874580	8.600371	-0.047957	4.497712
231.973272	6956.849050	8.605376	-0.047978	4.500209
232.214951	6964.860503	8.610381	-0.048028	4.502717
232.431278	6972.899710	8.615386	-0.048074	4.505232
232.609437	6980.907856	8.620391	-0.048113	4.507735
232.661519	6988.971554	8.625395	-0.048128	4.510254
232.605218	6996.990648	8.630400	-0.048123	4.512758
232.826892	7005.059039	8.635405	-0.048170	4.515276
233.097138	7013.022510	8.640410	-0.048225	4.517760
233.010724	7020.992135	8.645415	-0.048215	4.520244
233.216401	7029.005098	8.650419	-0.048258	4.522741
233.567269	7036.988453	8.655424	-0.048329	4.525227
233.850437	7045.024981	8.660429	-0.048387	4.527728
233.908698	7053.089665	8.665434	-0.048404	4.530237
234.121904	7061.047328	8.670439	-0.048449	4.532711
234.188034	7069.116912	8.675443	-0.048467	4.535218
234.513787	7077.067711	8.680448	-0.048533	4.537687
234.536702	7085.096213	8.685453	-0.048542	4.540178
234.527507	7093.137381	8.690458	-0.048546	4.542672
234.665760	7101.087457	8.695463	-0.048577	4.545136
234.878288	7109.171552	8.700467	-0.048622	4.547641
234.999437	7117.150727	8.705472	-0.048650	4.550112
235.142117	7125.228038	8.710477	-0.048682	4.552612
235.112858	7133.253113	8.715482	-0.048682	4.555094
235.208794	7141.242595	8.720487	-0.048706	4.557564
235.499144	7149.278067	8.725491	-0.048765	4.560047
235.484238	7157.251543	8.730496	-0.048768	4.562509
235.754466	7165.235286	8.735501	-0.048823	4.564973
236.007633	7173.295406	8.740506	-0.048876	4.567459
236.056785	7181.297944	8.745511	-0.048891	4.569926
236.178734	7189.392769	8.750515	-0.048919	4.572420
236.588991	7197.391773	8.755520	-0.049001	4.574884
236.635077	7205.349664	8.760525	-0.049015	4.577333
236.841754	7213.376372	8.765530	-0.049059	4.579802
236.903248	7221.400765	8.770535	-0.049075	4.582269
237.298954	7229.417536	8.775539	-0.049155	4.584733
237.415468	7237.470919	8.780544	-0.049182	4.587206
237.487264	7245.463675	8.785549	-0.049201	4.589659
237.891309	7253.545656	8.790554	-0.049281	4.592139
237.984524	7261.526742	8.795559	-0.049304	4.594586
238.113162	7269.596663	8.800563	-0.049333	4.597059
238.303897	7277.492473	8.805568	-0.049374	4.599477
238.543508	7285.533256	8.810573	-0.049424	4.601938
238.580793	7293.535743	8.815578	-0.049437	4.604387
238.734501	7301.546523	8.820583	-0.049471	4.606836
239.124238	7309.547225	8.825587	-0.049549	4.609281
238.977293	7317.617899	8.830592	-0.049527	4.611747
239.231686	7325.657020	8.835597	-0.049580	4.614201
239.470690	7333.684151	8.840602	-0.049630	4.616650
239.886580	7341.630712	8.845607	-0.049713	4.619073
239.928837	7349.732028	8.850611	-0.049726	4.621542
239.898051	7357.654150	8.855616	-0.049726	4.623956
240.018738	7365.683113	8.860621	-0.049754	4.626400
240.105915	7373.682475	8.865626	-0.049775	4.628835
240.131751	7381.707572	8.870631	-0.049785	4.631275
240.372242	7389.758818	8.875635	-0.049836	4.633723
240.474679	7397.777184	8.880640	-0.049860	4.636159
240.610952	7405.739204	8.885645	-0.049891	4.638576
240.889863	7413.816863	8.890650	-0.049948	4.641028
241.021696	7421.752387	8.895655	-0.049978	4.643435
240.948238	7429.807970	8.900659	-0.049970	4.645877
241.164805	7437.786103	8.905664	-0.050016	4.648295
241.809539	7445.806829	8.910669	-0.050141	4.650723
241.792457	7453.885688	8.915674	-0.050144	4.653169
241.793263	7461.928601	8.920679	-0.050149	4.655602
242.051294	7469.901228	8.925683	-0.050203	4.658012
242.097572	7477.909353	8.930688	-0.050217	4.660433
241.981503	7485.908636	8.935693	-0.050201	4.662849
242.193441	7493.921631	8.940698	-0.050246	4.665268
242.435263	7501.959700	8.945703	-0.050296	4.667693
242.668880	7509.991661	8.950707	-0.050345	4.670115
242.770444	7518.064576	8.955712	-0.050369	4.672549
242.822640	7526.095901	8.960717	-0.050385	4.674968
242.780243	7534.064569	8.965722	-0.050382	4.677368
242.868892	7542.002724	8.970727	-0.050404	4.679757
243.264730	7550.056679	8.975731	-0.050483	4.682179
243.417262	7558.006621	8.980736	-0.050517	4.684569
243.381172	7566.052087	8.985741	-0.050516	4.686986
243.696087	7574.097564	8.990746	-0.050580	4.689402
243.743725	7582.106137	8.995751	-0.050594	4.691806
243.972931	7590.096061	9.000755	-0.050642	4.694203
243.915788	7598.130981	9.005760	-0.050637	4.696612
244.121443	7606.097816	9.010765	-0.050681	4.699000
244.600076	7614.157212	9.015770	-0.050775	4.701413
244.566869	7622.090036	9.020775	-0.050774	4.703788
244.665034	7630.176011	9.025779	-0.050798	4.706208
244.816324	7638.211258	9.030784	-0.050832	4.708611
245.005046	7646.188291	9.035789	-0.050872	4.710995
245.098016	7654.306644	9.040794	-0.050895	4.713421
245.272633	7662.241665	9.045799	-0.050933	4.715790
245.423461	7670.251695	9.050803	-0.050967	4.718180
245.391242	7678.246501	9.055808	-0.050966	4.720566
245.377796	7686.289495	9.060813	-0.050969	4.722964
245.729604	7694.333546	9.065818	-0.051040	4.725360
245.816703	7702.310225	9.070823	-0.051062	4.727736
246.066436	7710.378478	9.075827	-0.051114	4.730138
246.265117	7718.384339	9.080832	-0.051156	4.732519
246.445653	7726.424589	9.085837	-0.051195	4.734910
246.530784	7734.439676	9.090842	-0.051216	4.737293
246.557469	7742.446688	9.095847	-0.051227	4.739672
246.597818	7750.449470	9.100851	-0.051240	4.742048
246.766573	7758.412394	9.105856	-0.051277	4.744411
246.987399	7766.446230	9.110861	-0.051323	4.746794
247.297718	7774.479902	9.115866	-0.051386	4.749175
247.106677	7782.499550	9.120871	-0.051356	4.751552
247.437301	7790.547990	9.125875	-0.051423	4.753935
247.554764	7798.569688	9.130880	-0.051451	4.756310
247.605763	7806.538745	9.135885	-0.051466	4.758668
247.714365	7814.576868	9.140890	-0.051491	4.761045
247.870268	7822.484417	9.145895	-0.051526	4.763382
248.241381	7830.566585	9.150899	-0.051600	4.765769
248.264609	7838.603171	9.155904	-0.051610	4.768142
248.269660	7846.608637	9.160909	-0.051616	4.770505
248.458198	7854.682881	9.165914	-0.051657	4.772887
248.454275	7862.669782	9.170919	-0.051662	4.775242
248.785795	7870.634332	9.175923	-0.051729	4.777588
249.134032	7878.673119	9.180928	-0.051799	4.779955
249.106612	7886.636690	9.185933	-0.051799	4.782300
249.168516	7894.678612	9.190938	-0.051816	4.784667
249.358839	7902.722096	9.195943	-0.051857	4.787032
249.342397	7910.738033	9.200947	-0.051860	4.789389
249.286933	7918.764798	9.205952	-0.051855	4.791748
249.521893	7926.764648	9.210957	-0.051904	4.794096
249.858762	7934.817889	9.215962	-0.051972	4.796459
250.009417	7942.757516	9.220967	-0.052006	4.798788
249.986907	7950.837930	9.225971	-0.052007	4.801158
250.361596	7958.766500	9.230976	-0.052082	4.803480
250.288348	7966.799752	9.235981	-0.052074	4.805834
250.516802	7974.802211	9.240986	-0.052122	4.808177
250.568911	7982.828265	9.245991	-0.052137	4.810526
250.912087	7990.247077	9.250995	-0.052206	4.812695
250.900990	7994.684566	9.256000	-0.052207	4.813992

251.031340	7997.183076	9.261005	-0.052233	4.814722
251.220854	7998.526355	9.266010	-0.052269	4.815114
251.383571	7998.970083	9.271015	-0.052300	4.815243
251.229396	7999.892452	9.276019	-0.052272	4.815513
251.190901	7999.874755	9.281024	-0.052265	4.815508
251.173098	7999.858463	9.286029	-0.052262	4.815504
251.205645	7999.910278	9.291034	-0.052269	4.815519
251.356782	7999.823053	9.296039	-0.052297	4.815493
251.468073	7999.854794	9.301043	-0.052318	4.815501
251.540710	7999.942509	9.306048	-0.052332	4.815527
251.442082	7999.852272	9.311053	-0.052313	4.815501
251.573507	7999.924926	9.316058	-0.052338	4.815521
251.538774	7999.858161	9.321063	-0.052332	4.815502
251.480021	7999.879649	9.326067	-0.052321	4.815508
251.839917	7999.909044	9.331072	-0.052388	4.815515
251.952350	7999.869247	9.336077	-0.052410	4.815503
251.870125	7999.890351	9.341082	-0.052395	4.815510
251.817809	7999.824367	9.346087	-0.052385	4.815491
251.945227	7999.874528	9.351091	-0.052409	4.815505
251.891770	7999.895034	9.356096	-0.052399	4.815511
251.927023	7999.884949	9.361101	-0.052406	4.815508
251.914183	7999.880486	9.366106	-0.052404	4.815507
252.073792	7999.879909	9.371111	-0.052434	4.815506
251.961718	7999.911206	9.376115	-0.052413	4.815515
251.947534	7999.878953	9.381120	-0.052411	4.815506
252.207129	7999.822336	9.386125	-0.052459	4.815488
252.242420	7999.898761	9.391130	-0.052466	4.815510
252.057167	7999.864781	9.396135	-0.052432	4.815501
252.050382	7999.911682	9.401139	-0.052431	4.815515
252.144308	7999.934597	9.406144	-0.052448	4.815521
252.200276	7999.919510	9.411149	-0.052459	4.815517
252.216428	7999.932609	9.416154	-0.052462	4.815520
252.097280	7999.874076	9.421159	-0.052440	4.815504
252.328194	7999.853303	9.426163	-0.052483	4.815497
252.376186	7999.908576	9.431168	-0.052493	4.815513
252.257091	7999.835091	9.436173	-0.052471	4.815492
252.317153	7999.885221	9.441178	-0.052482	4.815506
252.416636	7999.809968	9.446183	-0.052501	4.815483
252.547688	7999.907183	9.451187	-0.052525	4.815511
252.304966	7999.862651	9.456192	-0.052480	4.815499
252.337083	7999.827950	9.461197	-0.052487	4.815489
252.362509	7999.908487	9.466202	-0.052492	4.815513
252.406489	7999.837666	9.471207	-0.052500	4.815492
252.485630	7999.841115	9.476211	-0.052515	4.815492
252.580698	7999.919586	9.481216	-0.052533	4.815515
252.651571	7999.882314	9.486221	-0.052546	4.815503
252.640939	7999.890704	9.491226	-0.052545	4.815506
252.366332	7999.846718	9.496231	-0.052494	4.815494
252.555293	7999.940608	9.501235	-0.052529	4.815521
252.831782	7999.915241	9.506240	-0.052581	4.815512
252.552302	7999.833794	9.511245	-0.052529	4.815490
252.618895	7999.911800	9.516250	-0.052542	4.815512
252.566897	7999.882132	9.521255	-0.052532	4.815504
252.569090	7999.916365	9.526259	-0.052533	4.815514
252.611824	7999.902130	9.531264	-0.052541	4.815509
252.724178	7999.877284	9.536269	-0.052562	4.815502
252.695571	7999.878972	9.541274	-0.052557	4.815502
252.582932	7999.847245	9.546279	-0.052536	4.815493
252.840495	7999.854677	9.551283	-0.052584	4.815494
252.713852	7999.856899	9.556288	-0.052561	4.815496
252.901189	7999.831143	9.561293	-0.052596	4.815487
252.767723	7999.918696	9.566298	-0.052571	4.815513
252.779212	7999.856957	9.571303	-0.052574	4.815495
252.770095	7999.866439	9.576307	-0.052572	4.815498
252.972024	7999.885779	9.581312	-0.052610	4.815503
253.097375	7999.882507	9.586317	-0.052634	4.815501
253.158878	7999.902756	9.591322	-0.052645	4.815507
252.986678	7999.829470	9.596327	-0.052614	4.815486
252.979294	7999.890247	9.601331	-0.052612	4.815504
253.120416	7999.887232	9.606336	-0.052639	4.815503
253.004259	7999.857584	9.611341	-0.052617	4.815494
252.933935	7999.936557	9.616346	-0.052605	4.815518
252.898348	7999.881524	9.621351	-0.052598	4.815502
252.994621	7999.855347	9.626355	-0.052616	4.815494
252.956643	7999.869699	9.631360	-0.052609	4.815498
253.006843	7999.855585	9.636365	-0.052619	4.815494
253.112372	7999.976951	9.641370	-0.052639	4.815529
252.965909	7999.908357	9.646375	-0.052612	4.815509
252.823869	7999.855857	9.651379	-0.052586	4.815495
252.907796	7999.839091	9.656384	-0.052601	4.815489
252.991082	7999.803089	9.661389	-0.052617	4.815478
253.080309	7999.881466	9.666394	-0.052634	4.815501
253.124192	7999.823460	9.671399	-0.052642	4.815484
253.067468	7999.841777	9.676403	-0.052632	4.815489
253.146605	7999.876199	9.681408	-0.052647	4.815499
253.342998	7999.867680	9.686413	-0.052684	4.815496
253.129374	7999.915474	9.691418	-0.052644	4.815511
253.142072	7999.890067	9.696423	-0.052647	4.815503
253.076291	7999.868718	9.701427	-0.052635	4.815497
253.097750	7999.892585	9.706432	-0.052639	4.815504
252.794798	7999.848135	9.711437	-0.052583	4.815493
252.978288	7999.888535	9.716442	-0.052617	4.815503
252.842906	7999.872456	9.721447	-0.052592	4.815499
252.949407	7999.888101	9.726451	-0.052612	4.815503
252.858590	7999.968875	9.731456	-0.052596	4.815528
252.976277	7999.924892	9.736461	-0.052618	4.815514
253.023921	7999.967344	9.741466	-0.052627	4.815526
252.861355	7999.881398	9.746471	-0.052597	4.815502
253.045297	7999.859859	9.751475	-0.052631	4.815495
253.149642	7999.855175	9.756480	-0.052651	4.815493
253.133595	7999.831435	9.761485	-0.052648	4.815486
253.106316	7999.932473	9.766490	-0.052643	4.815516
253.361420	7999.849082	9.771495	-0.052691	4.815490
253.399686	7999.883904	9.776499	-0.052698	4.815500
253.244477	7999.903815	9.781504	-0.052670	4.815507
253.162634	7999.845890	9.786509	-0.052655	4.815490
253.331521	7999.904209	9.791514	-0.052686	4.815506
253.233975	7999.864183	9.796519	-0.052668	4.815495
253.363948	7999.850306	9.801523	-0.052693	4.815490
253.253544	7999.966007	9.806528	-0.052672	4.815525
253.254984	7999.878469	9.811533	-0.052673	4.815499
253.228529	7999.983793	9.816538	-0.052668	4.815530
253.231676	7999.932597	9.821543	-0.052669	4.815515
253.295375	7999.916568	9.826547	-0.052681	4.815510
253.237798	7999.939144	9.831552	-0.052671	4.815517
253.232933	7999.931607	9.836557	-0.052670	4.815515
253.444715	7999.935088	9.841562	-0.052710	4.815515
253.316952	7999.875343	9.846567	-0.052686	4.815498
253.252968	7999.931992	9.851571	-0.052674	4.815515
253.431930	7999.933869	9.856576	-0.052708	4.815514
253.391250	7999.889432	9.861581	-0.052700	4.815502
253.615288	7999.924088	9.866586	-0.052742	4.815511
253.622720	7999.883642	9.871591	-0.052744	4.815499
253.599450	7999.895030	9.876595	-0.052740	4.815502
253.583484	7999.915081	9.881600	-0.052737	4.815508
253.526547	7999.897080	9.886605	-0.052727	4.815503
253.357922	8000.000081	9.891610	-0.052696	4.815534
253.526685	7999.936639	9.896615	-0.052727	4.815515
253.600369	7999.949612	9.901619	-0.052741	4.815518
253.653227	7999.947291	9.906624	-0.052751	4.815517
253.486783	7999.876233	9.911629	-0.052720	4.815497
253.395078	7999.911067	9.916634	-0.052704	4.815508
253.446169	7999.867063	9.921639	-0.052713	4.815495
253.393270	7999.885442	9.926643	-0.052704	4.815500
253.459428	7999.907904	9.931648	-0.052716	4.815507
253.403254	7999.866418	9.936653	-0.052706	4.815495
253.439496	7999.955679	9.941658	-0.052713	4.815521
253.475957	7999.914640	9.946663	-0.052720	4.815508
253.503273	7999.911902	9.951667	-0.052725	4.815508
253.462522	7999.962522	9.956672	-0.052718	4.815523
253.554419	7999.816651	9.961677	-0.052735	4.815479
253.525517	7999.895234	9.966682	-0.052730	4.815503
253.428697	7999.864832	9.971687	-0.052712	4.815494
253.515835	7999.933564	9.976691	-0.052729	4.815514
253.783076	7999.975336	9.981696	-0.052779	4.815525
253.663959	7999.938161	9.986701	-0.052757	4.815514
253.598822	7999.957408	9.991706	-0.052745	4.815520
253.516170	7999.913353	9.996711	-0.052730	4.815508
253.551457	7999.908609	10.001715	-0.052736	4.815506
253.528142	7999.932812	10.006720	-0.052732	4.815513
253.598543	7999.865626	10.011725	-0.052746	4.815493
253.577054	7999.921902	10.016730	-0.052742	4.815510
253.335006	7999.857084	10.021735	-0.052697	4.815492
253.680699	7999.864891	10.026739	-0.052762	4.815493
253.819090	7999.893874	10.031744	-0.052788	4.815501
253.673176	7999.870146	10.036749	-0.052761	4.815494
253.660220	7999.921221	10.041754	-0.052758	4.815509
253.737699	7999.897941	10.046759	-0.052773	4.815502
253.597878	7999.840135	10.051763	-0.052747	4.815486
253.702523	7999.907017	10.056768	-0.052767	4.815505
253.623206	7999.875834	10.061773	-0.052752	4.815496
253.728110	7999.936312	10.066778	-0.052772	4.815513
253.530110	7999.913868	10.071783	-0.052735	4.815508
253.749208	7999.870475	10.076787	-0.052776	4.815494
253.685116	7999.928190	10.081792	-0.052765	4.815511
253.670689	7999.920497	10.086797	-0.052762	4.815509
253.799581	7999.968551	10.091802	-0.052787	4.815523
253.613385	7999.964457	10.096807	-0.052752	4.815522
253.497400	7999.930537	10.101811	-0.052731	4.815513
253.543120	7999.931304	10.106816	-0.052739	4.815513
253.787222	7999.877639	10.111821	-0.052785	4.815496
253.795414	7999.934400	10.116826	-0.052787	4.815513
253.580857	7999.866827	10.121831	-0.052747	4.815494
253.729547	7999.857528	10.126835	-0.052775	4.815490
253.893767	7999.916840	10.131840	-0.052806	4.815507
253.628872	7999.867669	10.136845	-0.052757	4.815494
253.760286	7999.995870	10.141850	-0.052781	4.815531
253.659589	7999.965404	10.146855	-0.052763	4.815522
253.863912	7999.899339	10.151859	-0.052801	4.815502
253.792013	7999.934497	10.156864	-0.052788	4.815513
253.739791	7999.901620	10.161869	-0.052778	4.815503
253.822322	7999.969210	10.166874	-0.052794	4.815523
253.623623	7999.937142	10.171879	-0.052757	4.815514
253.705517	7999.917139	10.176883	-0.052773	4.815508
253.902379	7999.991938	10.181888	-0.052810	4.815529
253.760852	7999.867882	10.186893	-0.052783	4.815493
254.018052	7999.934056	10.191898	-0.052832	4.815511
253.808298	7999.901807	10.196903	-0.052793	4.815503
253.948431	7999.874211	10.201907	-0.052819	4.815494
253.780278	7999.887502	10.206912	-0.052788	4.815499
253.861881	7999.950804	10.211917	-0.052803	4.815517
254.043847	7999.999726	10.216922	-0.052838	4.815530
253.761827	7999.925708	10.221927	-0.052785	4.815510
253.769637	7999.941876	10.226931	-0.052787	4.815515
253.944014	7999.951156	10.231936	-0.052820	4.815517
253.809717	7999.931889	10.236941	-0.052795	4.815512
253.782708	7999.948556	10.241946	-0.052790	4.815517
253.732088	7999.959496	10.246951	-0.052781	4.815520
253.938874	7999.953284	10.251955	-0.052819	4.815517
253.751324	7999.991891	10.256960	-0.052785	4.815529
253.878022	7999.925625	10.261965	-0.052809	4.815509
253.979276	7999.965751	10.266970	-0.052828	4.815521
253.881970	7999.917184	10.271975	-0.052810	4.815507
254.055243	7999.897607	10.276979	-0.052842	4.815500
254.077155	7999.994112	10.281984	-0.052847	4.815528
253.763642	7999.928123	10.286989	-0.052788	4.815511
253.987355	7999.951026	10.291994	-0.052830	4.815516
253.782690	7999.909248	10.296999	-0.052792	4.815505
253.851864	7999.885832	10.302003	-0.052805	4.815498
254.012450	7999.942949	10.307008	-0.052836	4.815514
253.989789	7999.862492	10.312013	-0.052831	4.815490
254.045282	7999.893325	10.317018	-0.052842	4.815499
253.904421	7999.833365	10.322023	-0.052816	4.815482
254.127303	7999.861594	10.327027	-0.052858	4.815489
253.965781	7999.888878	10.332032	-0.052828	4.815498
253.954965	7999.852406	10.337037	-0.052826	4.815488
254.067166	7999.878825	10.342042	-0.052847	4.815495
253.978246	7999.866710	10.347047	-0.052831	4.815492
254.234851	7999.938215	10.352051	-0.052879	4.815511
254.094136	7999.918843	10.357056	-0.052853	4.815506
254.179669	7999.944827	10.362061	-0.052869	4.815513
254.364802	7999.964964	10.367066	-0.052904	4.815518
254.014164	7999.929341	10.372071	-0.052839	4.815510
254.012820	7999.918658	10.377075	-0.052839	4.815507
254.168313	8000.023756	10.382080	-0.052868	4.815537
254.104175	7999.929803	10.387085	-0.052856	4.815509
254.047025	7999.957726	10.392090	-0.052846	4.815518
253.915588	7999.952391	10.397095	-0.052821	4.815517
254.172189	7999.912815	10.402099	-0.052869	4.815504
254.199381	7999.930369	10.407104	-0.052875	4.815509
254.102232	7999.904233	10.412109	-0.052857	4.815502
254.091446	8000.016225	10.417114	-0.052855	4.815535
254.107680	7999.923586	10.422119	-0.052858	4.815508
253.977474	7999.963131	10.427123	-0.052834	4.815520
254.197568	7999.934707	10.432128	-0.052875	4.815510
253.961545	7999.892415	10.437133	-0.052832	4.815499
253.902101	7999.924573	10.442138	-0.052821	4.815509
253.949921	7999.924306	10.447143	-0.052830	4.815508
254.125439	7999.906902	10.452147	-0.052863	4.815503
253.998752	7999.974275	10.457152	-0.052840	4.815523
253.890607	7999.863581	10.462157	-0.052820	4.815491
254.032751	7999.935350	10.467162	-0.052846	4.815511
254.129603	7999.878209	10.472167	-0.052865	4.815494
254.082546	7999.874254	10.477171	-0.052856	4.815493
254.259973	7999.925239	10.482176	-0.052889	4.815507
254.268610	7999.892288	10.487181	-0.052891	4.815498
254.192243	7999.909216	10.492186	-0.052877	4.815503
254.096994	7999.901269	10.497191	-0.052860	4.815501
254.187377	7999.896358	10.502195	-0.052877	4.815499
254.084730	7999.958783	10.507200	-0.052858	4.815518
254.156674	7999.892690	10.512205	-0.052871	4.815498
254.369927	7999.984848	10.517210	-0.052911	4.815524
254.213895	7999.970566	10.522215	-0.052882	4.815521
254.194987	7999.902986	10.527219	-0.052879	4.815501
254.271864	7999.961940	10.532224	-0.052894	4.815518
254.234323	7999.873762	10.537229	-0.052887	4.815492
254.330271	7999.940504	10.542234	-0.052905	4.815511
254.049220	7999.948743	10.547239	-0.052853	4.815515
254.369030	7999.971082	10.552243	-0.052913	4.815520
254.349705	8000.015645	10.557248	-0.052909	4.815533
254.055820	7999.947840	10.562253	-0.052855	4.815515
254.216429	7999.983597	10.567258	-0.052885	4.815524
254.185150	7999.910475	10.572263	-0.052879	4.815503
254.181066	7999.874112	10.577267	-0.052879	4.815493
254.290625	7999.921851	10.582272	-0.052899	4.815506
254.244470	7999.899753	10.587277	-0.052891	4.815500
254.230001	7999.911285	10.592282	-0.052888	4.815503
254.088276	7999.941029	10.597287	-0.052862	4.815513
254.089866	7999.937870	10.602291	-0.052863	4.815512
254.147065	7999.975139	10.607296	-0.052874	4.815522
253.991268	7999.878619	10.612301	-0.052845	4.815495
254.126571	7999.928915	10.617306	-0.052870	4.815509
254.198926	7999.954683	10.622311	-0.052884	4.815516
254.139631	7999.914213	10.627315	-0.052873	4.815504
254.030387	7999.990416	10.632320	-0.052853	4.815527
254.184128	7999.885073	10.637325	-0.052882	4.815496
254.393260	7999.882104	10.642330	-0.052921	4.815494
254.347958	7999.915561	10.647335	-0.052913	4.815504
254.262938	7999.964390	10.652339	-0.052897	4.815518
254.289502	8000.004363	10.657344	-0.052902	4.815530
254.221693	7999.918894	10.662349	-0.052890	4.815505
254.265722	7999.946335	10.667354	-0.052898	4.815513
254.273562	7999.931530	10.672359	-0.052900	4.815509
254.186487	7999.893810	10.677363	-0.052884	4.815498
254.246507	7999.940738	10.682368	-0.052895	4.815512
254.310715	7999.951420	10.687373	-0.052908	4.815514
254.347949	8000.019339	10.692378	-0.052915	4.815534
254.226058	7999.988525	10.697383	-0.052892	4.815526
254.211900	7999.948793	10.702387	-0.052890	4.815514
254.257280	7999.986938	10.707392	-0.052899	4.815525
254.212135	7999.938155	10.712397	-0.052890	4.815511
254.248137	7999.991099	10.717402	-0.052897	4.815526
254.441499	7999.928060	10.722407	-0.052934	4.815507
254.378930	7999.969779	10.727411	-0.052922	4.815519
254.348260	7999.984250	10.732416	-0.052917	4.815524
254.295750	7999.958844	10.737421	-0.052907	4.815517
254.520088	7999.982827	10.742426	-0.052949	4.815523
254.377248	7999.874768	10.747431	-0.052923	4.815492
254.394451	7999.879341	10.752435	-0.052926	4.815493
254.666195	7999.982070	10.757440	-0.052977	4.815522
254.412631	7999.906379	10.762445	-0.052930	4.815501
254.556512	7999.953612	10.767450	-0.052957	4.815514
254.539498	7999.906356	10.772455	-0.052954	4.815500
254.436297	7999.917504	10.777459	-0.052935	4.815504
254.560287	7999.974025	10.782464	-0.052958	4.815520
254.378282	7999.880279	10.787469	-0.052925	4.815493
254.495868	7999.917468	10.792474	-0.052947	4.815503
254.369678	7999.910083	10.797479	-0.052923	4.815502
254.365527	7999.877991	10.802483	-0.052923	4.815493
254.583189	7999.983040	10.807488	-0.052964	4.815522
254.516327	7999.933901	10.812493	-0.052951	4.815508
254.676543	7999.969652	10.817498	-0.052981	4.815518
254.674162	7999.918364	10.822503	-0.052981	4.815503
254.620248	7999.919637	10.827507	-0.052971	4.815503
254.388504	7999.920138	10.832512	-0.052928	4.815505
254.424831	7999.895117	10.837517	-0.052935	4.815497
254.449819	7999.951086	10.842522	-0.052940	4.815513
254.218257	7999.929160	10.847527	-0.052897	4.815508
254.252582	7999.907310	10.852531	-0.052904	4.815502
254.485793	7999.918621	10.857536	-0.052948	4.815504
254.474843	7999.875737	10.862541	-0.052946	4.815491
254.482361	7999.967735	10.867546	-0.052948	4.815518
254.343431	7999.932371	10.872551	-0.052922	4.815508
254.499414	7999.867652	10.877555	-0.052951	4.815489
254.686650	7999.945500	10.882560	-0.052986	4.815511
254.529114	7999.926921	10.887565	-0.052957	4.815506
254.461114	7999.985641	10.892570	-0.052945	4.815523
254.455665	7999.980231	10.897575	-0.052944	4.815522
254.503668	7999.950060	10.902579	-0.052953	4.815513
254.580212	8000.051733	10.907584	-0.052968	4.815542
254.320881	7999.932155	10.912589	-0.052919	4.815508
254.591494	7999.953691	10.917594	-0.052970	4.815513
254.469547	7999.976281	10.922599	-0.052948	4.815521
254.512836	7999.983417	10.927603	-0.052956	4.815523
254.517513	8000.011284	10.932608	-0.052957	4.815531
254.505058	7999.941672	10.937613	-0.052955	4.815510
254.513389	7999.988824	10.942618	-0.052957	4.815524
254.411673	7999.987179	10.947623	-0.052938	4.815524
254.319082	7999.953641	10.952627	-0.052921	4.815515
254.382823	7999.963248	10.957632	-0.052933	4.815517
254.488407	7999.934019	10.962637	-0.052953	4.815508
254.489739	7999.944741	10.967642	-0.052953	4.815511
254.434841	7999.942794	10.972647	-0.052943	4.815511
254.542506	7999.917872	10.977651	-0.052963	4.815503
254.437359	7999.975985	10.982656	-0.052944	4.815521
254.470322	7999.916730	10.987661	-0.052950	4.815503
254.620164	7999.937358	10.992666	-0.052979	4.815508
254.516038	7999.920720	10.997671	-0.052959	4.815504
254.586163	7999.902661	11.002675	-0.052973	4.815498
254.598067	7999.931713	11.007680	-0.052975	4.815507
254.677140	7999.917004	11.012685	-0.052990	4.815502
254.563779	7999.956825	11.017690	-0.052969	4.815514
254.604167	7999.939347	11.022695	-0.052977	4.815509
254.524543	7999.831254	11.027699	-0.052962	4.815478
254.544905	7999.966187	11.032704	-0.052966	4.815517
254.465158	7999.908292	11.037709	-0.052952	4.815501
254.590536	7999.934928	11.042714	-0.052975	4.815508
254.566098	7999.958046	11.047719	-0.052971	4.815515
254.430199	7999.939821	11.052723	-0.052946	4.815510
254.346208	7999.934193	11.057728	-0.052930	4.815509
254.633954	7999.873766	11.062733	-0.052984	4.815490
254.607869	7999.918218	11.067738	-0.052980	4.815503
254.521973	7999.977714	11.072743	-0.052964	4.815521
254.624589	7999.965527	11.077747	-0.052983	4.815517
254.811392	8000.025212	11.082752	-0.053018	4.815533
254.578396	7999.971218	11.087757	-0.052975	4.815518
254.795220	7999.904289	11.092762	-0.053016	4.815498
254.735730	7999.949264	11.097767	-0.053005	4.815511
254.598357	7999.955580	11.102771	-0.052979	4.815514
254.774733	7999.962758	11.107776	-0.053012	4.815515
254.593237	7999.970488	11.112781	-0.052979	4.815518
254.566587	7999.929484	11.117786	-0.052974	4.815506
254.551819	7999.951691	11.122791	-0.052972	4.815513
254.675056	7999.938773	11.127795	-0.052995	4.815508
254.587754	8000.003587	11.132800	-0.052979	4.815528
254.495821	7999.983944	11.137805	-0.052962	4.815523
254.609530	7999.961257	11.142810	-0.052983	4.815515
254.702689	8000.038636	11.147815	-0.053001	4.815537
254.704444	8000.040820	11.152819	-0.053001	4.815538
254.734694	8000.030653	11.157824	-0.053007	4.815535
254.705843	7999.952228	11.162829	-0.053002	4.815512
254.686072	7999.929494	11.167834	-0.052998	4.815506
254.575468	7999.967223	11.172839	-0.052978	4.815517
254.723877	7999.910925	11.177843	-0.053006	4.815500
254.703447	8000.008875	11.182848	-0.053002	4.815529
254.472821	7999.914333	11.187853	-0.052960	4.815502
254.629103	7999.921181	11.192858	-0.052989	4.815503
254.643938	7999.921443	11.197863	-0.052992	4.815503
254.714003	7999.920472	11.202867	-0.053005	4.815503
254.680576	8000.019278	11.207872	-0.052999	4.815532
254.780887	7999.992100	11.212877	-0.053018	4.815523
254.866041	8000.036237	11.217882	-0.053034	4.815536
254.678722	7999.948810	11.222887	-0.053000	4.815511
254.560188	7999.916984	11.227891	-0.052978	4.815503
254.678688	8000.007594	11.232896	-0.053000	4.815528
254.556599	7999.958619	11.237901	-0.052977	4.815515
254.819686	7999.974692	11.242906	-0.053027	4.815518
254.846208	8000.026414	11.247911	-0.053032	4.815533
254.661849	7999.961467	11.252915	-0.052998	4.815515
254.732431	7999.947687	11.257920	-0.053011	4.815511
254.779963	7999.947416	11.262925	-0.053020	4.815510
254.675227	7999.932904	11.267930	-0.053001	4.815507
254.499495	7999.948206	11.272935	-0.052968	4.815512
254.600951	7999.885799	11.277939	-0.052987	4.815493
254.701405	7999.997476	11.282944	-0.053006	4.815525
254.654856	7999.975372	11.287949	-0.052998	4.815519
254.698493	8000.002808	11.292954	-0.053006	4.815527
254.883356	8000.010124	11.297959	-0.053041	4.815528
254.752487	7999.977027	11.302963	-0.053017	4.815519
254.994509	8000.023731	11.307968	-0.053062	4.815532
254.928575	8000.031216	11.312973	-0.053050	4.815534
255.005140	8000.036760	11.317978	-0.053065	4.815535
254.852072	7999.991550	11.322983	-0.053036	4.815523
254.997924	7999.917052	11.327987	-0.053064	4.815500
255.153739	7999.990116	11.332992	-0.053093	4.815521
254.773832	7999.918764	11.337997	-0.053022	4.815502
254.804946	7999.945995	11.343002	-0.053028	4.815510
254.986654	7999.978895	11.348007	-0.053062	4.815518
254.911301	7999.945637	11.353011	-0.053049	4.815509
254.715419	7999.946724	11.358016	-0.053012	4.815510
254.799215	7999.944910	11.363021	-0.053028	4.815509
254.792916	7999.912783	11.368026	-0.053027	4.815500
254.592929	7999.926620	11.373031	-0.052990	4.815505
254.706728	7999.923160	11.378035	-0.053012	4.815503
254.841638	7999.988405	11.383040	-0.053037	4.815522
254.652238	7999.949010	11.388045	-0.053002	4.815511
254.734829	7999.924746	11.393050	-0.053017	4.815504
254.724166	7999.904296	11.398055	-0.053016	4.815498
254.743982	7999.866188	11.403059	-0.053019	4.815487
254.838059	8000.003396	11.408064	-0.053037	4.815526
254.793834	7999.931128	11.413069	-0.053029	4.815505
255.049335	7999.958826	11.418074	-0.053077	4.815512
255.039118	7999.983245	11.423079	-0.053075	4.815519
254.653702	7999.913940	11.428083	-0.053004	4.815501
254.891068	7999.913570	11.433088	-0.053048	4.815500
254.773706	7999.898852	11.438093	-0.053027	4.815496
254.874919	7999.913344	11.443098	-0.053046	4.815500
254.890386	7999.927502	11.448103	-0.053049	4.815504
254.657844	7999.923716	11.453107	-0.053006	4.815504
254.760243	7999.936092	11.458112	-0.053025	4.815507
254.703669	7999.851873	11.463117	-0.053015	4.815483
254.902750	7999.921372	11.468122	-0.053052	4.815502
254.926798	7999.931397	11.473127	-0.053057	4.815505
254.909713	7999.882004	11.478131	-0.053054	4.815490
255.042812	7999.933334	11.483136	-0.053079	4.815505
255.062096	7999.889876	11.488141	-0.053082	4.815492
254.952623	7999.934033	11.493146	-0.053062	4.815505
254.960661	7999.937388	11.498151	-0.053064	4.815506
255.007205	7999.942441	11.503155	-0.053073	4.815508
255.182410	8000.044663	11.508160	-0.053106	4.815537
254.865177	7999.971131	11.513165	-0.053047	4.815517
254.889581	7999.917076	11.518170	-0.053052	4.815501
255.103444	8000.007112	11.523175	-0.053092	4.815526
254.827546	7999.920371	11.528179	-0.053041	4.815502
254.968941	7999.959020	11.533184	-0.053067	4.815513
254.855647	7999.957185	11.538189	-0.053046	4.815513
254.825576	7999.905443	11.543194	-0.053041	4.815498
254.710194	7999.886485	11.548199	-0.053020	4.815493
254.813506	7999.862560	11.553203	-0.053039	4.815485
254.838543	7999.927075	11.558208	-0.053044	4.815504
254.889619	7999.969586	11.563213	-0.053054	4.815516
255.250772	7999.991537	11.568218	-0.053121	4.815521
255.022205	8000.027336	11.573223	-0.053079	4.815532
254.965271	7999.940974	11.578227	-0.053068	4.815507
255.112800	7999.926318	11.583232	-0.053096	4.815502
255.056248	7999.955319	11.588237	-0.053086	4.815511
254.854974	7999.962726	11.593242	-0.053049	4.815514
254.907289	7999.958260	11.598247	-0.053058	4.815513
254.885601	7999.891702	11.603251	-0.053055	4.815493
255.089693	7999.966624	11.608256	-0.053093	4.815514
254.965011	7999.947513	11.613261	-0.053070	4.815509
255.145888	7999.910972	11.618266	-0.053104	4.815498
255.143789	7999.996406	11.623271	-0.053104	4.815523
254.915307	7999.895488	11.628275	-0.053061	4.815494
254.917208	7999.968170	11.633280	-0.053062	4.815515
254.912948	7999.929667	11.638285	-0.053061	4.815504
254.978908	7999.911540	11.643290	-0.053074	4.815498
254.983795	7999.984271	11.648295	-0.053075	4.815520
254.918565	7999.895637	11.653299	-0.053063	4.815494
255.047573	8000.000306	11.658304	-0.053087	4.815524
255.000074	7999.987799	11.663309	-0.053079	4.815521
255.232380	7999.965985	11.668314	-0.053122	4.815513
255.141690	8000.017926	11.673319	-0.053105	4.815529
255.013755	7999.925061	11.678323	-0.053082	4.815502
254.913417	7999.986457	11.683328	-0.053063	4.815521
255.145090	7999.943271	11.688333	-0.053107	4.815507
255.024618	7999.933842	11.693338	-0.053084	4.815505
255.011711	7999.941126	11.698343	-0.053082	4.815507
255.060126	7999.935529	11.703347	-0.053091	4.815505
255.174089	7999.959844	11.708352	-0.053113	4.815512
254.978911	7999.954533	11.713357	-0.053077	4.815511
254.938351	7999.980591	11.718362	-0.053070	4.815519
255.225434	7999.944720	11.723367	-0.053123	4.815507
255.171274	7999.949193	11.728371	-0.053113	4.815508
255.278834	8000.036422	11.733376	-0.053134	4.815533
255.372918	8000.007006	11.738381	-0.053151	4.815524
255.172796	7999.962093	11.743386	-0.053114	4.815512
254.992992	8000.002963	11.748391	-0.053081	4.815525
254.984964	7999.910992	11.753395	-0.053080	4.815498
255.059142	7999.977380	11.758400	-0.053094	4.815517
254.793633	7999.946352	11.763405	-0.053044	4.815509
254.793898	7999.910060	11.768410	-0.053045	4.815499
254.880778	7999.977724	11.773415	-0.053061	4.815518
254.723567	7999.940991	11.778419	-0.053032	4.815508
254.763360	7999.966228	11.783424	-0.053040	4.815515
254.866590	7999.928416	11.788429	-0.053059	4.815504
255.045559	8000.002927	11.793434	-0.053093	4.815525
254.913676	8000.005061	11.798439	-0.053068	4.815526
254.946582	7999.916965	11.803443	-0.053075	4.815500
255.202480	7999.966032	11.808448	-0.053123	4.815513
255.051549	7999.946492	11.813453	-0.053095	4.815508
255.139065	7999.922308	11.818458	-0.053111	4.815501
255.060875	7999.995816	11.823463	-0.053097	4.815523
255.107388	7999.934646	11.828467	-0.053106	4.815504
254.939392	7999.977845	11.833472	-0.053075	4.815518
255.148858	7999.984496	11.838477	-0.053114	4.815519
255.175428	7999.969996	11.843482	-0.053119	4.815514
255.093477	7999.980424	11.848487	-0.053104	4.815518
255.147715	7999.935401	11.853491	-0.053114	4.815504
255.026218	7999.979361	11.858496	-0.053092	4.815518
255.139829	7999.969490	11.863501	-0.053113	4.815514
255.075710	7999.959915	11.868506	-0.053102	4.815512
255.094845	7999.996564	11.873511	-0.053105	4.815523
255.105484	7999.952964	11.878515	-0.053108	4.815510
255.183955	7999.975630	11.883520	-0.053122	4.815516
255.228747	7999.994540	11.888525	-0.053131	4.815521
255.279243	7999.978296	11.893530	-0.053141	4.815516
255.143727	8000.023095	11.898535	-0.053116	4.815530
254.997724	7999.972659	11.903539	-0.053089	4.815516
255.273371	8000.045549	11.908544	-0.053140	4.815536
255.288332	7999.987066	11.913549	-0.053143	4.815519
255.269029	7999.942976	11.918554	-0.053140	4.815506
255.352327	8000.000970	11.923559	-0.053156	4.815523
255.260069	7999.924710	11.928563	-0.053139	4.815501
255.243789	7999.982142	11.933568	-0.053136	4.815518
255.059034	7999.993023	11.938573	-0.053102	4.815522
255.287672	7999.933764	11.943578	-0.053144	4.815503
255.156025	8000.010670	11.948583	-0.053120	4.815526
255.172169	7999.988523	11.953587	-0.053123	4.815520
255.088691	8000.045923	11.958592	-0.053108	4.815537
254.965423	7999.974497	11.963597	-0.053085	4.815517
255.108312	7999.960832	11.968602	-0.053112	4.815512
255.394463	8000.003987	11.973607	-0.053166	4.815523
255.140630	7999.937901	11.978611	-0.053118	4.815505
255.285480	8000.030013	11.983616	-0.053146	4.815531
255.233127	7999.974701	11.988621	-0.053136	4.815515
255.197465	7999.933548	11.993626	-0.053130	4.815503
255.212528	7999.973334	11.998631	-0.053133	4.815515
255.254394	7999.930246	12.003635	-0.053141	4.815502
255.275370	7999.934880	12.008640	-0.053145	4.815503
255.220428	7999.968180	12.013645	-0.053135	4.815513
255.059818	7999.899348	12.018650	-0.053105	4.815494
255.184863	7999.953751	12.023655	-0.053129	4.815509
255.101212	7999.910745	12.028659	-0.053113	4.815497
255.005732	7999.969016	12.033664	-0.053096	4.815515
254.836178	7999.903242	12.038669	-0.053064	4.815496
254.919817	7999.901425	12.043674	-0.053080	4.815495
255.197679	7999.962602	12.048679	-0.053132	4.815512
255.171871	7999.905588	12.053683	-0.053128	4.815495
255.372400	7999.935592	12.058688	-0.053165	4.815503
255.226080	8000.020803	12.063693	-0.053138	4.815529
255.127803	7999.904925	12.068698	-0.053120	4.815495
255.484956	7999.924674	12.073703	-0.053187	4.815499
255.030163	7999.916183	12.078707	-0.053102	4.815499
255.274980	7999.905254	12.083712	-0.053148	4.815495
255.253229	7999.916667	12.088717	-0.053144	4.815498
255.456576	7999.905060	12.093722	-0.053182	4.815494
255.222421	7999.935427	12.098727	-0.053139	4.815504
255.140065	7999.866807	12.103731	-0.053124	4.815484
255.377453	7999.897414	12.108736	-0.053168	4.815492
255.132119	7999.910508	12.113741	-0.053123	4.815497
255.282710	7999.911924	12.118746	-0.053151	4.815497
255.428192	7999.973071	12.123751	-0.053178	4.815514
255.150921	7999.986710	12.128755	-0.053127	4.815519
255.006482	7999.923483	12.133760	-0.053100	4.815501
255.187786	7999.937150	12.138765	-0.053134	4.815504
255.041080	7999.967880	12.143770	-0.053107	4.815514
255.129266	8000.014204	12.148775	-0.053124	4.815527
254.924518	7999.943581	12.153779	-0.053086	4.815508
255.438414	7999.971236	12.158784	-0.053182	4.815513
255.208035	7999.910874	12.163789	-0.053139	4.815497
255.172560	7999.868656	12.168794	-0.053133	4.815484
255.346795	7999.948432	12.173799	-0.053165	4.815507
255.312915	7999.892354	12.178803	-0.053159	4.815491
255.259203	7999.933151	12.183808	-0.053150	4.815503
255.321208	7999.997204	12.188813	-0.053161	4.815521
255.219672	7999.944291	12.193818	-0.053143	4.815506
255.240558	8000.011944	12.198823	-0.053147	4.815526
255.030496	7999.857921	12.203827	-0.053108	4.815482
255.323796	7999.909737	12.208832	-0.053163	4.815496
255.472272	8000.006181	12.213837	-0.053191	4.815523
255.186486	7999.885098	12.218842	-0.053137	4.815489
255.375893	7999.956576	12.223847	-0.053173	4.815509
255.261671	7999.913069	12.228851	-0.053152	4.815497
255.394182	7999.982549	12.233856	-0.053177	4.815517
255.296115	7999.971350	12.238861	-0.053159	4.815514
255.426837	7999.968168	12.243866	-0.053183	4.815512
255.306537	7999.946992	12.248871	-0.053161	4.815507
255.312072	7999.969533	12.253875	-0.053162	4.815513
255.183793	7999.937545	12.258880	-0.053139	4.815504
255.307416	7999.986585	12.263885	-0.053162	4.815518
255.147360	7999.954077	12.268890	-0.053132	4.815509
255.249494	7999.989948	12.273895	-0.053152	4.815519
255.420360	7999.887019	12.278899	-0.053184	4.815488
255.436183	7999.934294	12.283904	-0.053187	4.815502
255.292302	7999.981093	12.288909	-0.053160	4.815517
255.259073	7999.903663	12.293914	-0.053154	4.815494
255.470040	8000.020357	12.298919	-0.053194	4.815527
255.231862	7999.935300	12.303923	-0.053150	4.815503
255.407448	8000.040733	12.308928	-0.053183	4.815533
255.329025	8000.030924	12.313933	-0.053168	4.815531
255.238148	7999.971776	12.318938	-0.053152	4.815514
255.147275	8000.046145	12.323943	-0.053135	4.815536
255.016373	8000.000229	12.328947	-0.053111	4.815523
255.212564	7999.982096	12.333952	-0.053147	4.815517
255.158954	7999.986579	12.338957	-0.053138	4.815519
255.294904	7999.949302	12.343962	-0.053163	4.815507
255.419630	7999.967385	12.348967	-0.053187	4.815512
255.164271	7999.895933	12.353971	-0.053139	4.815492
255.182477	7999.943247	12.358976	-0.053143	4.815506
255.354160	7999.973848	12.363981	-0.053175	4.815514
255.183468	7999.896305	12.368986	-0.053143	4.815492
255.421467	8000.021986	12.373991	-0.053188	4.815528
255.514454	8000.006437	12.378995	-0.053206	4.815523
255.515003	7999.978693	12.384000	-0.053206	4.815515
255.506156	7999.986045	12.389005	-0.053204	4.815517
255.499262	7999.929340	12.394010	-0.053203	4.815500
255.418931	8000.045539	12.399015	-0.053189	4.815535
255.261132	7999.982092	12.404019	-0.053159	4.815517
255.344127	7999.999491	12.409024	-0.053175	4.815522
255.519242	8000.000241	12.414029	-0.053208	4.815521
255.376787	7999.954135	12.419034	-0.053182	4.815508
255.433525	8000.018102	12.424039	-0.053192	4.815527
255.376393	7999.995824	12.429043	-0.053182	4.815520
255.511449	8000.019416	12.434048	-0.053207	4.815527
255.441454	8000.004404	12.439053	-0.053195	4.815523
255.372440	7999.971249	12.444058	-0.053182	4.815513
255.441862	8000.034357	12.449063	-0.053195	4.815531
255.430275	7999.971166	12.454067	-0.053193	4.815513
255.381556	7999.992819	12.459072	-0.053184	4.815519
255.347511	7999.946351	12.464077	-0.053178	4.815506
255.487712	7999.929439	12.469082	-0.053204	4.815500
255.505784	7999.985297	12.474087	-0.053208	4.815517
255.541539	7999.966675	12.479091	-0.053215	4.815511
255.515379	7999.950244	12.484096	-0.053210	4.815506
255.401632	7999.972968	12.489101	-0.053189	4.815513
255.476334	7999.987027	12.494106	-0.053203	4.815517
255.516168	8000.052855	12.499111	-0.053211	4.815536
255.336184	7999.943115	12.504115	-0.053178	4.815505
255.410744	7999.990284	12.509120	-0.053192	4.815518
255.244506	7999.957675	12.514125	-0.053161	4.815510
255.314428	7999.922522	12.519130	-0.053174	4.815499
255.347272	8000.009597	12.524135	-0.053181	4.815524
255.535540	7999.957155	12.529139	-0.053216	4.815508
255.427388	7999.908406	12.534144	-0.053196	4.815494
255.431014	7999.944801	12.539149	-0.053197	4.815505
255.381184	7999.887394	12.544154	-0.053188	4.815488
255.615593	7999.930771	12.549159	-0.053232	4.815500
255.329422	7999.874836	12.554163	-0.053179	4.815485
255.466334	7999.921957	12.559168	-0.053204	4.815498
255.464762	8000.006333	12.564173	-0.053204	4.815523
255.495239	7999.901106	12.569178	-0.053210	4.815492
255.382267	7999.986863	12.574183	-0.053189	4.815518
255.228110	7999.915999	12.579187	-0.053161	4.815498
255.455824	7999.963538	12.584192	-0.053204	4.815510
255.595232	7999.993611	12.589197	-0.053230	4.815518
255.377202	7999.922769	12.594202	-0.053189	4.815499
255.463349	7999.982945	12.599207	-0.053206	4.815516
255.387119	7999.937923	12.604211	-0.053192	4.815503
255.507782	7999.979438	12.609216	-0.053214	4.815515
255.701746	7999.968747	12.614221	-0.053251	4.815511
255.498582	7999.917374	12.619226	-0.053213	4.815497
255.404625	7999.997034	12.624231	-0.053196	4.815520
255.635756	8000.004041	12.629235	-0.053239	4.815521
255.686955	7999.973922	12.634240	-0.053249	4.815512
255.443141	8000.001994	12.639245	-0.053204	4.815522
255.542352	7999.959844	12.644250	-0.053222	4.815509
255.557157	7999.998558	12.649255	-0.053225	4.815520
255.525503	7999.935039	12.654259	-0.053220	4.815502
255.351380	7999.984547	12.659264	-0.053187	4.815517
255.603210	7999.998302	12.664269	-0.053235	4.815520
255.677597	7999.930109	12.669274	-0.053249	4.815499
255.597464	7999.974747	12.674279	-0.053234	4.815513
255.525808	7999.940481	12.679283	-0.053221	4.815503
255.676290	7999.935486	12.684288	-0.053249	4.815501
255.617384	7999.970858	12.689293	-0.053238	4.815512
255.568347	7999.903850	12.694298	-0.053229	4.815492
255.710794	7999.956403	12.699303	-0.053256	4.815507
255.676154	7999.945174	12.704307	-0.053250	4.815504
255.567983	7999.976535	12.709312	-0.053230	4.815513
255.447066	8000.004482	12.714317	-0.053208	4.815522
255.630432	7999.930597	12.719322	-0.053242	4.815500
255.698301	8000.018247	12.724327	-0.053255	4.815525
255.577739	7999.974635	12.729331	-0.053233	4.815513
255.816264	7999.987104	12.734336	-0.053277	4.815515
255.568184	7999.954222	12.739341	-0.053231	4.815507
255.340847	7999.937703	12.744346	-0.053189	4.815503
255.510778	8000.012068	12.749351	-0.053221	4.815524
255.669186	7999.965546	12.754355	-0.053251	4.815510
255.663939	7999.902460	12.759360	-0.053250	4.815491
255.498214	7999.932878	12.764365	-0.053219	4.815501
255.657587	7999.894917	12.769370	-0.053249	4.815489
255.729558	7999.948453	12.774375	-0.053263	4.815504
255.499429	7999.921206	12.779379	-0.053220	4.815498
255.554061	7999.973390	12.784384	-0.053231	4.815513
255.620166	7999.995854	12.789389	-0.053243	4.815519
255.602064	7999.967805	12.794394	-0.053240	4.815511
255.520300	7999.969691	12.799399	-0.053225	4.815512
255.473639	7999.927289	12.804403	-0.053216	4.815499
255.535007	7999.971038	12.809408	-0.053228	4.815512
255.628057	7999.959763	12.814413	-0.053246	4.815508
255.709843	7999.888487	12.819418	-0.053261	4.815487
255.599906	7999.930500	12.824423	-0.053241	4.815500
255.596171	7999.936867	12.829427	-0.053240	4.815502
255.483940	7999.968162	12.834432	-0.053220	4.815511
255.604872	7999.925299	12.839437	-0.053242	4.815498
255.574038	7999.971811	12.844442	-0.053237	4.815512
255.509635	7999.998547	12.849447	-0.053225	4.815520
255.532485	7999.939125	12.854451	-0.053230	4.815503
255.662489	7999.998952	12.859456	-0.053254	4.815519
255.426889	7999.985501	12.864461	-0.053210	4.815517
255.468111	7999.961628	12.869466	-0.053218	4.815509
255.642350	7999.980521	12.874471	-0.053251	4.815514
255.501564	7999.906671	12.879475	-0.053225	4.815493
255.733241	7999.952140	12.884480	-0.053268	4.815505
255.662779	7999.988390	12.889485	-0.053255	4.815516
255.768703	7999.914306	12.894490	-0.053275	4.815494
255.729490	7999.974567	12.899495	-0.053268	4.815512
255.536733	7999.891320	12.904499	-0.053233	4.815488
255.681021	7999.911860	12.909504	-0.053260	4.815494
255.569127	7999.944228	12.914509	-0.053239	4.815504
255.429434	7999.909916	12.919514	-0.053213	4.815494
255.695103	7999.974100	12.924519	-0.053263	4.815512
255.475633	7999.940619	12.929523	-0.053222	4.815503
255.688700	7999.988987	12.934528	-0.053262	4.815516
255.822034	8000.032847	12.939533	-0.053287	4.815528
255.618390	7999.946217	12.944538	-0.053250	4.815504
255.659459	8000.003520	12.949543	-0.053257	4.815521
255.907457	7999.937102	12.954547	-0.053304	4.815500
255.801486	7999.953545	12.959552	-0.053284	4.815505
255.745462	7999.981486	12.964557	-0.053274	4.815514
255.789057	7999.893564	12.969562	-0.053282	4.815488
255.656220	7999.958701	12.974567	-0.053258	4.815508
255.556829	7999.966706	12.979571	-0.053240	4.815510
255.496532	7999.988169	12.984576	-0.053229	4.815517
255.716106	8000.003533	12.989581	-0.053270	4.815520
255.548258	7999.989055	12.994586	-0.053239	4.815517
255.465652	8000.074241	12.999591	-0.053224	4.815542
255.455394	7999.975823	13.004595	-0.053222	4.815513
255.528730	7999.983452	13.009600	-0.053236	4.815515
255.392551	8000.015422	13.014605	-0.053211	4.815525
255.530851	7999.913028	13.019610	-0.053237	4.815495
255.849965	7999.984496	13.024615	-0.053296	4.815514
255.532939	7999.986802	13.029619	-0.053237	4.815516
255.520970	7999.942831	13.034624	-0.053235	4.815503
255.643511	7999.993991	13.039629	-0.053258	4.815518
255.578453	7999.916039	13.044634	-0.053246	4.815495
255.578071	7999.959846	13.049639	-0.053247	4.815508
255.615985	7999.975440	13.054643	-0.053254	4.815513
255.729439	7999.987997	13.059648	-0.053275	4.815516
255.674197	7999.994589	13.064653	-0.053265	4.815518
255.619378	7999.917873	13.069658	-0.053255	4.815496
255.688994	7999.985257	13.074663	-0.053268	4.815515
255.558567	7999.998095	13.079667	-0.053244	4.815519
255.500462	8000.014253	13.084672	-0.053234	4.815524
255.543141	8000.030993	13.089677	-0.053242	4.815529
255.708532	7999.942928	13.094682	-0.053273	4.815503
255.732161	8000.020240	13.099687	-0.053278	4.815525
255.476053	7999.960523	13.104691	-0.053230	4.815509
255.652926	7999.975187	13.109696	-0.053263	4.815512
255.699272	7999.939648	13.114701	-0.053272	4.815502
255.511683	7999.891735	13.119706	-0.053237	4.815488
255.846681	8000.006189	13.124711	-0.053300	4.815520
255.951367	7999.926743	13.129715	-0.053320	4.815497
255.702718	7999.996393	13.134720	-0.053274	4.815518
255.647382	8000.022210	13.139725	-0.053264	4.815526
255.765630	7999.982507	13.144730	-0.053286	4.815514
255.702249	8000.054123	13.149735	-0.053274	4.815535
255.625825	7999.989870	13.154739	-0.053260	4.815517
255.716507	8000.019146	13.159744	-0.053277	4.815525
255.807747	8000.053771	13.164749	-0.053294	4.815534
255.666773	7999.966031	13.169754	-0.053268	4.815509
255.688663	8000.031565	13.174759	-0.053273	4.815528
255.566607	8000.017836	13.179763	-0.053250	4.815525
255.647215	8000.013834	13.184768	-0.053265	4.815523
255.469147	8000.037642	13.189773	-0.053233	4.815531
255.842773	7999.983962	13.194778	-0.053302	4.815514
255.997739	8000.037790	13.199783	-0.053331	4.815529
255.738876	8000.023957	13.204787	-0.053283	4.815526
255.737457	7999.989772	13.209792	-0.053283	4.815516
255.746319	8000.042276	13.214797	-0.053285	4.815531
255.681695	7999.989966	13.219802	-0.053273	4.815516
255.774671	8000.082300	13.224807	-0.053291	4.815543
255.819168	8000.043526	13.229811	-0.053299	4.815531
255.523765	8000.013073	13.234816	-0.053245	4.815524
255.517900	7999.999111	13.239821	-0.053244	4.815520
255.644962	7999.993733	13.244826	-0.053268	4.815518
255.696570	8000.064027	13.249831	-0.053277	4.815538
255.735831	8000.009145	13.254835	-0.053285	4.815522
255.639740	7999.972342	13.259840	-0.053267	4.815511
255.732503	8000.020878	13.264845	-0.053285	4.815525
255.625507	7999.986033	13.269850	-0.053265	4.815515
255.856616	8000.059266	13.274855	-0.053308	4.815536
255.686822	8000.016984	13.279859	-0.053277	4.815524
255.836192	7999.992745	13.284864	-0.053305	4.815516
255.900678	8000.051500	13.289869	-0.053317	4.815533
255.689231	7999.993581	13.294874	-0.053278	4.815517
255.667911	8000.069090	13.299879	-0.053274	4.815539
255.532196	7999.983572	13.304883	-0.053249	4.815515
255.555189	7999.935901	13.309888	-0.053254	4.815501
255.687415	7999.966925	13.314893	-0.053279	4.815509
255.581999	7999.937447	13.319898	-0.053259	4.815501
255.631806	7999.945758	13.324903	-0.053269	4.815503
255.552976	7999.947691	13.329907	-0.053254	4.815504
255.568222	7999.957573	13.334912	-0.053257	4.815507
255.591421	8000.030606	13.339917	-0.053262	4.815528
255.647313	7999.917249	13.344922	-0.053272	4.815495
255.684636	7999.989445	13.349927	-0.053280	4.815516
255.456862	7999.993212	13.354931	-0.053237	4.815518
255.581019	7999.934380	13.359936	-0.053261	4.815500
255.726277	7999.999797	13.364941	-0.053288	4.815519
255.769486	7999.962071	13.369946	-0.053296	4.815508
255.628330	7999.979006	13.374951	-0.053270	4.815513
255.641188	7999.945055	13.379955	-0.053273	4.815503
255.707365	7999.947225	13.384960	-0.053285	4.815503
255.631016	7999.966289	13.389965	-0.053271	4.815509
255.667755	7999.928457	13.394970	-0.053278	4.815498
255.833517	7999.966439	13.399975	-0.053309	4.815508
255.818775	7999.958739	13.404979	-0.053307	4.815506
255.922971	7999.936965	13.409984	-0.053327	4.815499
255.818157	7999.997221	13.414989	-0.053307	4.815518
255.601198	7999.882602	13.419994	-0.053267	4.815485
255.721663	8000.018110	13.424999	-0.053290	4.815524
255.723455	8000.032045	13.430003	-0.053290	4.815528
255.665642	8000.002278	13.435008	-0.053280	4.815520
255.711640	8000.028685	13.440013	-0.053289	4.815527
255.816565	7999.933221	13.445018	-0.053308	4.815499
255.905095	8000.000915	13.450023	-0.053325	4.815518
255.719995	7999.975472	13.455027	-0.053291	4.815512
256.041681	7999.941237	13.460032	-0.053351	4.815500
256.028923	7999.995523	13.465037	-0.053349	4.815516
255.927507	7999.915907	13.470042	-0.053330	4.815493
255.837974	8000.034093	13.475047	-0.053314	4.815528
255.935698	7999.959873	13.480051	-0.053332	4.815506
255.889539	7999.916411	13.485056	-0.053324	4.815493
255.722500	7999.955353	13.490061	-0.053293	4.815506
255.876230	7999.913027	13.495066	-0.053322	4.815493
255.945282	8000.007105	13.500071	-0.053335	4.815520
255.712200	7999.955242	13.505075	-0.053291	4.815506
255.703226	7999.901707	13.510080	-0.053290	4.815490
255.837114	7999.989370	13.515085	-0.053315	4.815515
255.888134	7999.980611	13.520090	-0.053325	4.815512
255.951418	7999.985939	13.525095	-0.053337	4.815513
255.988097	7999.972673	13.530099	-0.053344	4.815509
255.955436	7999.972157	13.535104	-0.053338	4.815509
256.004840	8000.013575	13.540109	-0.053348	4.815521
255.826858	7999.945523	13.545114	-0.053315	4.815502
255.955342	8000.027757	13.550119	-0.053339	4.815526
255.948736	8000.008441	13.555123	-0.053338	4.815520
255.741556	7999.981569	13.560128	-0.053299	4.815513
255.698485	8000.058858	13.565133	-0.053292	4.815536
255.679847	7999.966711	13.570138	-0.053288	4.815509
255.822687	8000.011795	13.575143	-0.053315	4.815522
255.667860	7999.945190	13.580147	-0.053286	4.815503
255.724732	7999.903415	13.585152	-0.053297	4.815490
255.747366	7999.973234	13.590157	-0.053302	4.815511
255.697847	7999.976715	13.595162	-0.053293	4.815512
255.802274	8000.008352	13.600167	-0.053312	4.815521
255.823089	7999.976668	13.605171	-0.053316	4.815511
255.831356	7999.952255	13.610176	-0.053318	4.815504
255.857717	7999.990091	13.615181	-0.053323	4.815515
255.783707	7999.917332	13.620186	-0.053310	4.815494
255.842167	8000.020851	13.625191	-0.053321	4.815524
255.831299	7999.976898	13.630195	-0.053319	4.815511
255.891154	8000.003533	13.635200	-0.053330	4.815519
255.762225	8000.037758	13.640205	-0.053307	4.815529
255.609246	7999.974388	13.645210	-0.053278	4.815512
255.839497	8000.008085	13.650215	-0.053322	4.815520
255.677264	8000.021470	13.655219	-0.053292	4.815525
255.510592	8000.037987	13.660224	-0.053261	4.815531
255.636961	8000.050757	13.665229	-0.053284	4.815534
255.603317	8000.024590	13.670234	-0.053278	4.815526
255.689073	8000.016400	13.675239	-0.053295	4.815523
255.639239	7999.960059	13.680243	-0.053286	4.815507
255.691726	7999.966279	13.685248	-0.053296	4.815509
255.867413	8000.027923	13.690253	-0.053328	4.815526
255.896869	7999.975016	13.695258	-0.053334	4.815510
256.083750	8000.012277	13.700263	-0.053369	4.815520
255.964501	7999.982571	13.705267	-0.053347	4.815512
255.888036	7999.922590	13.710272	-0.053333	4.815495
255.853374	7999.955154	13.715277	-0.053327	4.815505
255.961622	7999.935583	13.720282	-0.053347	4.815498
256.028641	8000.003993	13.725287	-0.053360	4.815518
255.894969	7999.955893	13.730291	-0.053335	4.815505
256.081663	7999.934401	13.735296	-0.053370	4.815498
255.967328	7999.967798	13.740301	-0.053349	4.815508
255.852144	7999.929614	13.745306	-0.053328	4.815497
255.892951	8000.024298	13.750311	-0.053336	4.815525
255.914608	7999.999036	13.755315	-0.053340	4.815517
255.800098	8000.037770	13.760320	-0.053319	4.815529
255.805876	8000.043225	13.765325	-0.053320	4.815531
255.986050	7999.983173	13.770330	-0.053354	4.815512
255.845021	7999.963793	13.775335	-0.053328	4.815507
255.780333	7999.996934	13.780339	-0.053316	4.815517
256.010760	7999.928092	13.785344	-0.053359	4.815496
255.660474	7999.986465	13.790349	-0.053294	4.815515
255.793183	7999.902137	13.795354	-0.053319	4.815489
255.852949	7999.924497	13.800359	-0.053331	4.815496
256.023988	7999.966838	13.805363	-0.053363	4.815507
255.764650	7999.901727	13.810368	-0.053315	4.815489
255.799245	7999.967470	13.815373	-0.053321	4.815508
255.803855	7999.917361	13.820378	-0.053322	4.815494
256.080976	7999.965712	13.825383	-0.053374	4.815507
255.787096	7999.911785	13.830387	-0.053320	4.815492
255.743975	7999.905757	13.835392	-0.053312	4.815491
255.948067	7999.980684	13.840397	-0.053350	4.815512
255.690230	7999.898507	13.845402	-0.053302	4.815489
255.872036	7999.903639	13.850407	-0.053336	4.815489
256.030489	7999.934024	13.855411	-0.053366	4.815498
256.024089	7999.893349	13.860416	-0.053365	4.815486
256.037573	7999.935246	13.865421	-0.053368	4.815498
256.187815	7999.916363	13.870426	-0.053396	4.815492
256.010825	7999.976505	13.875431	-0.053363	4.815510
255.895447	7999.971430	13.880435	-0.053342	4.815509
256.222420	7999.893487	13.885440	-0.053403	4.815485
256.116603	7999.933432	13.890445	-0.053384	4.815497
255.827480	7999.912695	13.895450	-0.053330	4.815492
255.926571	7999.927154	13.900455	-0.053349	4.815496
255.873855	7999.975445	13.905459	-0.053339	4.815510
255.947157	7999.902962	13.910464	-0.053353	4.815489
255.960229	7999.965148	13.915469	-0.053356	4.815507
255.915163	7999.961225	13.920474	-0.053347	4.815506
256.008401	7999.933931	13.925479	-0.053365	4.815498
255.999850	8000.028876	13.930483	-0.053364	4.815525
255.875983	7999.948892	13.935488	-0.053341	4.815503
255.952780	7999.962986	13.940493	-0.053355	4.815506
255.867483	7999.926360	13.945498	-0.053340	4.815496
256.032063	7999.957914	13.950503	-0.053370	4.815504
256.071893	7999.935086	13.955507	-0.053378	4.815498
256.068760	7999.911554	13.960512	-0.053378	4.815491
255.884416	7999.939531	13.965517	-0.053344	4.815500
255.928561	7999.874048	13.970522	-0.053352	4.815480
256.051697	7999.852584	13.975527	-0.053375	4.815473
255.771118	7999.935598	13.980531	-0.053323	4.815499
255.862271	7999.905065	13.985536	-0.053340	4.815490
255.952313	7999.877718	13.990541	-0.053357	4.815481
255.757012	7999.870268	13.995546	-0.053321	4.815480
255.917920	7999.917783	14.000551	-0.053351	4.815493
255.984969	7999.940263	14.005555	-0.053364	4.815499
255.944842	7999.879809	14.010560	-0.053357	4.815482
255.975051	7999.971116	14.015565	-0.053363	4.815508
255.964141	7999.894049	14.020570	-0.053361	4.815486
255.968924	7999.981735	14.025575	-0.053362	4.815512
255.872863	7999.928910	14.030579	-0.053344	4.815497
255.909845	7999.918853	14.035584	-0.053351	4.815493
256.090671	7999.986991	14.040589	-0.053385	4.815513
255.955277	7999.899341	14.045594	-0.053360	4.815488
256.008805	7999.907713	14.050599	-0.053370	4.815490
256.157101	7999.913365	14.055603	-0.053398	4.815491
255.943353	7999.921634	14.060608	-0.053359	4.815494
255.756839	7999.970939	14.065613	-0.053324	4.815509
255.830841	7999.945466	14.070618	-0.053338	4.815502
255.857217	7999.964076	14.075623	-0.053343	4.815507
255.766887	7999.935912	14.080627	-0.053327	4.815499
255.671859	7999.932239	14.085632	-0.053309	4.815498
256.018084	8000.042606	14.090637	-0.053374	4.815529
255.763866	7999.974374	14.095642	-0.053327	4.815510
255.907109	7999.934012	14.100647	-0.053354	4.815498
256.057958	7999.921547	14.105651	-0.053382	4.815493
256.073908	7999.939986	14.110656	-0.053385	4.815499
255.868225	7999.949455	14.115661	-0.053347	4.815503
256.037625	7999.966134	14.120666	-0.053379	4.815507
256.105680	7999.970472	14.125671	-0.053392	4.815508
255.984691	7999.928989	14.130675	-0.053369	4.815496
255.931130	7999.927063	14.135680	-0.053360	4.815496
255.967517	7999.929814	14.140685	-0.053367	4.815496
255.988856	7999.905615	14.145690	-0.053371	4.815489
256.053420	7999.956894	14.150695	-0.053383	4.815504
255.758551	7999.930723	14.155699	-0.053328	4.815498
256.040092	7999.928943	14.160704	-0.053381	4.815496
256.087609	7999.992761	14.165709	-0.053390	4.815514
256.000658	7999.904836	14.170714	-0.053374	4.815489
256.074566	7999.950928	14.175719	-0.053388	4.815502
255.933766	8000.015935	14.180723	-0.053362	4.815522
255.866451	7999.976398	14.185728	-0.053350	4.815510
256.033631	8000.020813	14.190733	-0.053381	4.815523
256.122831	7999.904796	14.195738	-0.053398	4.815488
256.094418	7999.948144	14.200743	-0.053393	4.815501
256.095952	7999.998392	14.205747	-0.053393	4.815516
256.106506	7999.949449	14.210752	-0.053396	4.815501
256.129727	8000.001120	14.215757	-0.053400	4.815516
256.069489	7999.983062	14.220762	-0.053389	4.815511
256.063826	7999.941330	14.225767	-0.053388	4.815499
256.061049	7999.950917	14.230771	-0.053388	4.815502
255.969311	7999.898163	14.235776	-0.053371	4.815487
256.057070	7999.991481	14.240781	-0.053388	4.815514
256.010073	7999.903142	14.245786	-0.053379	4.815488
255.897976	7999.918416	14.250791	-0.053359	4.815493
256.144702	7999.975883	14.255795	-0.053405	4.815509
256.022598	7999.174941	14.260800	-0.053382	4.815275

255.906072	7995.964791	14.265805	-0.053358	4.814337
255.844937	7990.581457	14.270810	-0.053343	4.812764
256.047900	7983.882999	14.275815	-0.053377	4.810803
256.026181	7976.624728	14.280819	-0.053369	4.808679
255.799818	7968.994395	14.285824	-0.053322	4.806447
255.984830	7961.189693	14.290829	-0.053351	4.804160
255.928509	7953.338102	14.295834	-0.053336	4.801859
255.803601	7945.389197	14.300839	-0.053308	4.799529
255.725198	7937.454476	14.305843	-0.053288	4.797202
255.610604	7929.380596	14.310848	-0.053262	4.794833
255.666837	7921.430163	14.315853	-0.053267	4.792498
255.651206	7913.323189	14.320858	-0.053259	4.790117
255.729335	7905.404242	14.325863	-0.053269	4.787789
255.577585	7897.309729	14.330867	-0.053236	4.785410
255.357288	7889.398727	14.335872	-0.053190	4.783083
255.687292	7881.388815	14.340877	-0.053246	4.780724
255.622069	7873.371119	14.345882	-0.053229	4.778363
255.495683	7865.440305	14.350887	-0.053200	4.776027
255.402829	7857.375154	14.355891	-0.053178	4.773650
255.376339	7849.354066	14.360896	-0.053168	4.771284
255.192877	7841.352989	14.365901	-0.053129	4.768924
255.150560	7833.377781	14.370906	-0.053116	4.766570
255.128648	7825.328588	14.375911	-0.053107	4.764192
255.147567	7817.440234	14.380915	-0.053106	4.761861
255.186478	7809.356457	14.385920	-0.053108	4.759471
255.098096	7801.420871	14.390925	-0.053086	4.757124
255.171283	7793.357144	14.395930	-0.053095	4.754737
255.108254	7785.333871	14.400935	-0.053078	4.752362
254.824482	7777.301682	14.405939	-0.053020	4.749983
254.705123	7769.279619	14.410944	-0.052993	4.747606
254.790863	7761.334319	14.415949	-0.053004	4.745249
254.686303	7753.327843	14.420954	-0.052980	4.742874
254.825987	7745.352102	14.425959	-0.053001	4.740506
254.931662	7737.385216	14.430963	-0.053015	4.738139
254.648244	7729.334425	14.435968	-0.052958	4.735748
254.686013	7721.322405	14.440973	-0.052960	4.733366
254.739942	7713.304072	14.445978	-0.052965	4.730981
254.750868	7705.304055	14.450983	-0.052962	4.728600
254.444558	7697.311492	14.455987	-0.052900	4.726221
254.488925	7689.270653	14.460992	-0.052903	4.723825
254.643083	7681.336413	14.465997	-0.052927	4.721460
254.424852	7673.268971	14.471002	-0.052881	4.719055
254.470049	7665.342865	14.476007	-0.052884	4.716690
254.331023	7657.340816	14.481011	-0.052854	4.714302
254.387555	7649.297397	14.486016	-0.052859	4.711899
254.140975	7641.275581	14.491021	-0.052808	4.709503
254.047452	7633.282068	14.496026	-0.052786	4.707113
254.342832	7625.276715	14.501031	-0.052836	4.704718
254.228704	7617.331869	14.506035	-0.052810	4.702341
254.125890	7609.312991	14.511040	-0.052785	4.699940
254.207394	7601.357843	14.516045	-0.052796	4.697556
254.148810	7593.254798	14.521050	-0.052780	4.695128
254.129026	7585.286324	14.526055	-0.052771	4.692738
254.127681	7577.274184	14.531059	-0.052766	4.690334
254.154181	7569.263207	14.536064	-0.052766	4.687929
254.001629	7561.308308	14.541069	-0.052732	4.685540
253.782027	7553.295879	14.546074	-0.052686	4.683133
253.650524	7545.315126	14.551079	-0.052657	4.680734
253.640122	7537.300759	14.556083	-0.052650	4.678323
253.700281	7529.306442	14.561088	-0.052656	4.675917
253.778637	7521.247903	14.566093	-0.052666	4.673490
253.447273	7513.130525	14.571098	-0.052599	4.671045
253.730376	7505.197292	14.576103	-0.052647	4.668653
253.582463	7497.234130	14.581107	-0.052614	4.666252
253.439071	7489.169646	14.586112	-0.052582	4.663818
253.370383	7481.258590	14.591117	-0.052565	4.661430
253.598040	7473.230767	14.596122	-0.052602	4.659005
253.595668	7465.265123	14.601127	-0.052597	4.656598
253.263977	7457.218932	14.606131	-0.052530	4.654165
253.358538	7449.230996	14.611136	-0.052543	4.651748
253.273602	7441.216769	14.616141	-0.052522	4.649322
253.403436	7433.225886	14.621146	-0.052541	4.646902
253.369295	7425.197518	14.626151	-0.052530	4.644470
253.179647	7417.257445	14.631155	-0.052489	4.642062
253.111989	7409.194232	14.636160	-0.052472	4.639617
253.299670	7401.270510	14.641165	-0.052502	4.637212
253.091109	7393.165144	14.646170	-0.052458	4.634751
253.171098	7385.171446	14.651175	-0.052468	4.632322
253.196453	7377.188008	14.656179	-0.052467	4.629895
252.982421	7369.208489	14.661184	-0.052423	4.627469
252.881288	7361.203604	14.666189	-0.052399	4.625033
252.880563	7353.193828	14.671194	-0.052394	4.622594
252.830259	7345.180064	14.676199	-0.052379	4.620153
252.979549	7337.214665	14.681203	-0.052402	4.617726
252.943709	7329.155119	14.686208	-0.052390	4.615268
253.055539	7321.218548	14.691213	-0.052406	4.612846
252.837306	7313.091923	14.696218	-0.052360	4.610366
252.834946	7305.175074	14.701223	-0.052355	4.607948
252.804551	7297.146991	14.706227	-0.052344	4.605494
252.722307	7289.179395	14.711232	-0.052324	4.603058
252.715579	7281.200674	14.716237	-0.052318	4.600618
252.566720	7273.193740	14.721242	-0.052285	4.598167
252.367102	7265.190193	14.726247	-0.052243	4.595716
252.530410	7257.134392	14.731251	-0.052268	4.593247
252.224725	7249.097966	14.736256	-0.052206	4.590784
252.316594	7241.123186	14.741261	-0.052219	4.588337
252.278459	7233.090879	14.746266	-0.052206	4.585872
252.365492	7225.142915	14.751271	-0.052218	4.583432
252.224066	7217.175366	14.756275	-0.052186	4.580984
252.172839	7209.118475	14.761280	-0.052172	4.578507
252.221284	7201.154979	14.766285	-0.052176	4.576058
252.144990	7193.134259	14.771290	-0.052157	4.573590
252.251332	7185.088911	14.776295	-0.052171	4.571113
252.197968	7177.133563	14.781299	-0.052157	4.568662
252.108898	7169.102648	14.786304	-0.052135	4.566187
252.182169	7161.164555	14.791309	-0.052144	4.563739
251.980567	7153.174177	14.796314	-0.052101	4.561273
252.047715	7145.136497	14.801319	-0.052109	4.558791
252.083698	7137.193244	14.806323	-0.052110	4.556338
251.922747	7129.122895	14.811328	-0.052075	4.553843
251.882233	7121.119028	14.816333	-0.052063	4.551368
251.715976	7113.052591	14.821338	-0.052027	4.548872
251.673423	7105.084772	14.826343	-0.052014	4.546406
251.627085	7097.098147	14.831347	-0.052000	4.543932
251.657733	7089.129559	14.836352	-0.052001	4.541462
251.684207	7081.141169	14.841357	-0.052001	4.538985
251.796735	7073.154603	14.846362	-0.052017	4.536508
251.807606	7065.095580	14.851367	-0.052014	4.534006
251.741543	7057.100794	14.856371	-0.051997	4.531523
251.391677	7049.060084	14.861376	-0.051926	4.529023
251.509943	7041.148238	14.866381	-0.051943	4.526563
251.471404	7033.074215	14.871386	-0.051931	4.524051
251.510861	7025.178602	14.876391	-0.051934	4.521594
251.484396	7017.135439	14.881395	-0.051924	4.519089
251.523183	7009.169373	14.886400	-0.051926	4.516606
251.238069	7001.124119	14.891405	-0.051868	4.514097
251.095625	6992.998278	14.896410	-0.051836	4.511562
251.071321	6984.996089	14.901415	-0.051827	4.509064
251.169146	6977.071277	14.906419	-0.051840	4.506589
251.073454	6969.023605	14.911424	-0.051817	4.504074
250.921291	6961.114733	14.916429	-0.051784	4.501601
251.160613	6953.055115	14.921434	-0.051823	4.499080
250.972653	6945.066662	14.926439	-0.051783	4.496579
250.790536	6937.070721	14.931443	-0.051745	4.494074
250.791056	6929.034746	14.936448	-0.051740	4.491556
250.952763	6921.069404	14.941453	-0.051765	4.489059
250.766547	6913.054192	14.946458	-0.051725	4.486544
250.844561	6905.025964	14.951463	-0.051735	4.484024
250.705931	6897.112784	14.956467	-0.051704	4.481538
250.518331	6889.036718	14.961472	-0.051664	4.479000
250.669224	6881.114554	14.966477	-0.051687	4.476510
250.566232	6873.041773	14.971482	-0.051663	4.473969
250.630096	6865.014409	14.976487	-0.051670	4.471443
250.493436	6857.047341	14.981491	-0.051639	4.468933
250.674131	6849.023721	14.986496	-0.051668	4.466405
250.586002	6841.038406	14.991501	-0.051646	4.463887
250.399790	6833.059793	14.996506	-0.051607	4.461369
250.422028	6825.038758	15.001511	-0.051606	4.458837
250.442455	6817.048980	15.006515	-0.051605	4.456314
250.407996	6808.999230	15.011520	-0.051593	4.453769
250.231266	6800.998343	15.016525	-0.051555	4.451239
250.143219	6793.019687	15.021530	-0.051534	4.448714
250.068477	6785.011909	15.026535	-0.051515	4.446179
250.044505	6777.019888	15.031539	-0.051506	4.443647
249.892226	6769.024313	15.036544	-0.051472	4.441112
250.039680	6761.051927	15.041549	-0.051495	4.438585
249.769993	6753.037659	15.046554	-0.051440	4.436041
249.843983	6744.983967	15.051559	-0.051448	4.433484
249.835303	6736.956706	15.056563	-0.051442	4.430934
249.876269	6728.929434	15.061568	-0.051444	4.428383
249.950146	6720.982847	15.066573	-0.051453	4.425856
249.770917	6712.969977	15.071578	-0.051415	4.423305
249.784912	6705.013807	15.076583	-0.051412	4.420772
249.587439	6697.026219	15.081587	-0.051371	4.418226
249.517572	6688.980657	15.086592	-0.051353	4.415661
249.757616	6680.991740	15.091597	-0.051392	4.413114
249.670095	6672.945026	15.096602	-0.051371	4.410546
249.617462	6664.945490	15.101607	-0.051356	4.407991
249.546893	6656.965563	15.106611	-0.051338	4.405441
249.514904	6648.988686	15.111616	-0.051327	4.402891
249.565558	6641.045332	15.116621	-0.051332	4.400350
249.398634	6633.004876	15.121626	-0.051296	4.397775
249.211695	6625.001701	15.126631	-0.051256	4.395211
249.251775	6616.995500	15.131635	-0.051258	4.392646
249.192941	6608.941168	15.136640	-0.051242	4.390063
249.128990	6600.979251	15.141645	-0.051225	4.387508
249.074742	6592.954746	15.146650	-0.051210	4.384932
249.037549	6585.012418	15.151655	-0.051198	4.382381
249.007200	6576.986240	15.156659	-0.051188	4.379801
248.940412	6568.988771	15.161664	-0.051170	4.377229
249.067615	6561.001185	15.166669	-0.051189	4.374659
248.975112	6552.993264	15.171674	-0.051167	4.372081
249.072112	6544.967166	15.176679	-0.051180	4.369496
248.926020	6537.015287	15.181683	-0.051148	4.366932
248.787767	6528.972193	15.186688	-0.051117	4.364337
248.944837	6521.036523	15.191693	-0.051141	4.361777
248.866499	6512.978628	15.196698	-0.051121	4.359174
248.772965	6505.063051	15.201703	-0.051099	4.356616
248.680903	6496.981265	15.206707	-0.051077	4.354002
248.613392	6488.883620	15.211712	-0.051059	4.351382
248.545981	6480.929731	15.216717	-0.051042	4.348807
248.547718	6472.920382	15.221722	-0.051037	4.346213
248.409229	6464.937034	15.226727	-0.051006	4.343625
248.558713	6456.983266	15.231731	-0.051029	4.341047
248.361211	6448.966487	15.236736	-0.050987	4.338445
248.602625	6440.990411	15.241741	-0.051027	4.335857
248.477109	6432.968311	15.246746	-0.050999	4.333250
248.405116	6424.946092	15.251751	-0.050981	4.330642
248.379384	6416.985303	15.256755	-0.050971	4.328052
248.177602	6408.964143	15.261760	-0.050928	4.325440
248.246211	6400.995551	15.266765	-0.050936	4.322846
248.170726	6392.938225	15.271770	-0.050917	4.320220
248.281794	6385.002214	15.276775	-0.050933	4.317634
248.056918	6376.969554	15.281779	-0.050886	4.315011
247.903801	6368.936393	15.286784	-0.050852	4.312388
248.119898	6360.940674	15.291789	-0.050888	4.309778
247.983084	6352.942731	15.296794	-0.050857	4.307163
248.054506	6344.926642	15.301799	-0.050865	4.304542
248.000628	6336.990895	15.306803	-0.050850	4.301945
247.893931	6328.936370	15.311808	-0.050825	4.299307
247.811623	6320.979604	15.316813	-0.050805	4.296699
247.793352	6312.900473	15.321818	-0.050797	4.294051
247.861778	6304.902223	15.326823	-0.050804	4.291428
247.798705	6296.966311	15.331827	-0.050788	4.288822
247.725406	6288.928127	15.336832	-0.050769	4.286182
247.794459	6280.922681	15.341837	-0.050777	4.283551
247.733077	6272.922601	15.346842	-0.050761	4.280920
247.416562	6264.949186	15.351847	-0.050697	4.278294
247.471602	6257.010074	15.356851	-0.050702	4.275680
247.522114	6248.905396	15.361856	-0.050706	4.273011
247.454802	6240.893119	15.366861	-0.050689	4.270369
247.571297	6232.888551	15.371866	-0.050705	4.267730
247.319847	6224.903408	15.376871	-0.050654	4.265092
247.242883	6216.924311	15.381875	-0.050634	4.262456
246.997991	6208.921663	15.386880	-0.050584	4.259809
247.060715	6200.935557	15.391885	-0.050590	4.257169
246.970767	6192.908574	15.396890	-0.050569	4.254512
246.912534	6184.899915	15.401895	-0.050553	4.251860
246.991661	6176.867977	15.406899	-0.050562	4.249200
247.144784	6168.885109	15.411904	-0.050586	4.246555
247.011791	6160.940615	15.416909	-0.050556	4.243918
246.927234	6152.960254	15.421914	-0.050536	4.241268
246.979599	6144.947186	15.426919	-0.050540	4.238608
247.124865	6136.971216	15.431923	-0.050562	4.235958
246.945650	6128.946685	15.436928	-0.050524	4.233288
246.990483	6120.922651	15.441933	-0.050527	4.230618
246.850544	6112.941892	15.446938	-0.050496	4.227960
246.743292	6104.895935	15.451943	-0.050471	4.225278
246.642871	6096.964462	15.456947	-0.050448	4.222633
246.723158	6088.900695	15.461952	-0.050458	4.219943
246.502609	6081.001618	15.466957	-0.050412	4.217304
246.444682	6072.972783	15.471962	-0.050396	4.214622
246.423854	6064.920881	15.476967	-0.050387	4.211930
246.480465	6056.914693	15.481971	-0.050392	4.209253
246.067815	6048.922465	15.486976	-0.050311	4.206574
246.562118	6040.962333	15.491981	-0.050398	4.203914
246.170177	6032.989094	15.496986	-0.050320	4.201238
246.180124	6024.969376	15.501991	-0.050317	4.198549
246.425924	6016.997571	15.506995	-0.050357	4.195877
246.536230	6008.882609	15.512000	-0.050373	4.193153
246.253044	6000.832856	15.517005	-0.050315	4.190446
246.137727	5992.875861	15.522010	-0.050289	4.187770
246.112995	5984.898804	15.527015	-0.050279	4.185086
246.128769	5976.928342	15.532019	-0.050277	4.182403
245.680628	5968.911491	15.537024	-0.050189	4.179698
245.935778	5960.948126	15.542029	-0.050231	4.177017
245.943408	5952.894345	15.547034	-0.050227	4.174301
245.815358	5944.922471	15.552039	-0.050199	4.171609
245.808012	5936.933266	15.557043	-0.050192	4.168911
245.693250	5928.915003	15.562048	-0.050166	4.166200
245.763487	5920.945573	15.567053	-0.050174	4.163506
245.667002	5912.929784	15.572058	-0.050151	4.160793
245.596943	5904.909145	15.577063	-0.050133	4.158076
245.758570	5896.929079	15.582067	-0.050158	4.155375
245.479581	5888.900400	15.587072	-0.050101	4.152649
245.456111	5880.884751	15.592077	-0.050092	4.149930
245.690129	5872.880961	15.597082	-0.050130	4.147216
245.679567	5864.890039	15.602087	-0.050123	4.144501
245.597036	5856.951907	15.607091	-0.050103	4.141802
245.530145	5848.901904	15.612096	-0.050086	4.139063
245.656607	5840.961276	15.617101	-0.050104	4.136362
245.483032	5832.889999	15.622106	-0.050067	4.133611
245.317262	5824.871510	15.627111	-0.050031	4.130876
245.505044	5816.904081	15.632115	-0.050061	4.128161
245.172844	5808.906014	15.637120	-0.049994	4.125427
245.103518	5800.967678	15.642125	-0.049976	4.122715
245.236040	5792.927573	15.647130	-0.049996	4.119970
245.024818	5784.938438	15.652135	-0.049952	4.117235
244.866386	5776.941783	15.657139	-0.049917	4.114497
245.069336	5768.862187	15.662144	-0.049950	4.111733
245.205269	5760.850597	15.667149	-0.049970	4.108990
244.976039	5752.871844	15.672154	-0.049922	4.106251
245.049315	5744.842385	15.677159	-0.049931	4.103497
245.078084	5736.931813	15.682163	-0.049931	4.100781
244.883868	5728.904268	15.687168	-0.049890	4.098021
244.604120	5720.912771	15.692173	-0.049833	4.095270
244.627557	5712.938535	15.697178	-0.049833	4.092527
244.611410	5704.904107	15.702183	-0.049825	4.089761
244.728941	5696.947778	15.707187	-0.049842	4.087022
244.384262	5688.907290	15.712192	-0.049772	4.084245
244.521253	5680.989886	15.717197	-0.049793	4.081516
244.405037	5672.960360	15.722202	-0.049766	4.078743
244.215525	5664.973626	15.727207	-0.049726	4.075981
244.294803	5656.966199	15.732211	-0.049736	4.073214
244.270381	5648.930493	15.737216	-0.049726	4.070435
244.170371	5640.963784	15.742221	-0.049703	4.067676
244.172665	5632.945180	15.747226	-0.049698	4.064898
244.152441	5624.937491	15.752231	-0.049689	4.062123
244.083489	5616.937302	15.757235	-0.049671	4.059347
244.078501	5608.993020	15.762240	-0.049665	4.056590
244.255175	5600.943238	15.767245	-0.049693	4.053796
244.100067	5592.932588	15.772250	-0.049659	4.051010
244.079878	5584.967609	15.777255	-0.049651	4.048239
244.032422	5576.963517	15.782259	-0.049637	4.045453
243.934104	5568.962645	15.787264	-0.049614	4.042665
243.840749	5560.951011	15.792269	-0.049591	4.039872
243.836054	5553.012753	15.797274	-0.049585	4.037103
243.848424	5544.937030	15.802279	-0.049583	4.034285
243.563812	5536.852985	15.807283	-0.049525	4.031457
243.477723	5528.868808	15.812288	-0.049504	4.028665
243.566676	5520.888818	15.817293	-0.049515	4.025876
243.364447	5512.935114	15.822298	-0.049473	4.023089
243.567578	5504.923723	15.827303	-0.049505	4.020287
243.679240	5496.982439	15.832307	-0.049521	4.017505
243.519546	5488.919841	15.837312	-0.049486	4.014675
243.380502	5480.930553	15.842317	-0.049456	4.011869
243.486777	5472.934155	15.847322	-0.049470	4.009062
243.534952	5464.928172	15.852327	-0.049474	4.006249
243.520025	5456.934199	15.857331	-0.049467	4.003438
243.429034	5448.958173	15.862336	-0.049445	4.000629
243.451537	5440.988825	15.867341	-0.049444	3.997823
243.464452	5432.936958	15.872346	-0.049441	3.994985
243.319372	5424.898073	15.877351	-0.049409	3.992148
243.149245	5416.912108	15.882355	-0.049373	3.989326
243.143204	5408.924267	15.887360	-0.049366	3.986505
243.087221	5400.931169	15.892365	-0.049351	3.983679
242.879026	5392.990591	15.897370	-0.049307	3.980867
242.879951	5384.988594	15.902375	-0.049302	3.978035
242.944453	5376.973447	15.907379	-0.049309	3.975197
242.950090	5368.920123	15.912384	-0.049305	3.972342
243.074466	5360.902145	15.917389	-0.049324	3.969500
243.118979	5352.954339	15.922394	-0.049327	3.966680
242.901542	5344.936857	15.927399	-0.049281	3.963828
242.750490	5336.994921	15.932403	-0.049248	3.961003
242.778408	5328.975512	15.937408	-0.049249	3.958150
242.731965	5321.018959	15.942413	-0.049235	3.955317
242.637086	5312.963613	15.947418	-0.049212	3.952446
242.846823	5304.921171	15.952423	-0.049246	3.949582
242.657625	5297.002020	15.957427	-0.049206	3.946754
242.386842	5288.964150	15.962432	-0.049151	3.943879
242.464932	5281.018963	15.967437	-0.049160	3.941042
242.298019	5273.005215	15.972442	-0.049124	3.938174
242.251386	5265.013196	15.977447	-0.049110	3.935313
242.310488	5257.013881	15.982451	-0.049116	3.932450
242.232699	5248.963667	15.987456	-0.049097	3.929564
242.419962	5241.009616	15.992461	-0.049127	3.926715
242.296219	5233.004814	15.997466	-0.049099	3.923841
242.321321	5225.034010	16.002471	-0.049099	3.920979
242.198315	5217.073097	16.007475	-0.049071	3.918116
241.986479	5209.034963	16.012480	-0.049026	3.915221
241.951986	5201.002432	16.017485	-0.049015	3.912329
242.112309	5192.990945	16.022490	-0.049040	3.909447
241.968498	5185.023556	16.027495	-0.049008	3.906572
241.952618	5177.039879	16.032499	-0.049000	3.903692
242.102804	5168.998117	16.037504	-0.049023	3.900792
241.907566	5161.015776	16.042509	-0.048982	3.897905
241.716581	5153.038352	16.047514	-0.048941	3.895017
241.680283	5144.997529	16.052519	-0.048929	3.892108
241.819765	5136.989643	16.057523	-0.048950	3.889211
241.862322	5129.016935	16.062528	-0.048953	3.886323
241.717653	5121.040324	16.067533	-0.048921	3.883428
241.862823	5113.024123	16.072538	-0.048943	3.880522
241.655245	5105.056873	16.077543	-0.048900	3.877625
241.569891	5097.057312	16.082547	-0.048879	3.874716
241.608661	5088.781638	16.087552	-0.048881	3.871707
241.558292	5080.868775	16.092557	-0.048866	3.868826
241.438642	5072.929620	16.097562	-0.048839	3.865932
241.297870	5064.932555	16.102567	-0.048808	3.863014
241.507760	5056.988238	16.107571	-0.048842	3.860121
241.242143	5048.993901	16.112576	-0.048788	3.857197
241.281479	5040.998298	16.117581	-0.048790	3.854277
241.090487	5033.037728	16.122586	-0.048749	3.851362
241.113713	5024.974125	16.127591	-0.048749	3.848412
241.073269	5017.025082	16.132595	-0.048736	3.845501
240.945676	5009.035016	16.137600	-0.048708	3.842570
240.980631	5001.041120	16.142605	-0.048709	3.839639
241.064638	4993.082014	16.147610	-0.048720	3.836720
240.787951	4985.054185	16.152615	-0.048663	3.833765
240.796462	4977.055530	16.157619	-0.048660	3.830825
240.884978	4969.043188	16.162624	-0.048671	3.827880
240.964530	4961.069708	16.167629	-0.048681	3.824946
240.778194	4953.133662	16.172634	-0.048641	3.822018
240.669942	4945.089259	16.177639	-0.048616	3.819050
240.645697	4937.145262	16.182643	-0.048607	3.816118
240.734949	4929.079964	16.187648	-0.048618	3.813141
240.696709	4921.084919	16.192653	-0.048606	3.810186
240.583679	4913.118182	16.197658	-0.048580	3.807237
240.309868	4905.092046	16.202663	-0.048524	3.804260
240.520552	4897.145803	16.207667	-0.048558	3.801321
240.237625	4889.119376	16.212672	-0.048501	3.798339
240.434240	4881.128233	16.217677	-0.048532	3.795378
240.405481	4873.081809	16.222682	-0.048522	3.792390
240.365283	4865.055024	16.227687	-0.048510	3.789406
240.267787	4857.118561	16.232691	-0.048486	3.786453
240.175099	4849.103365	16.237696	-0.048464	3.783467
240.342639	4841.125827	16.242701	-0.048490	3.780500
240.108161	4833.149413	16.247706	-0.048442	3.777521
239.870217	4825.160369	16.252711	-0.048392	3.774535
240.161770	4817.118058	16.257715	-0.048442	3.771539
239.981954	4809.115709	16.262720	-0.048403	3.768544
239.935278	4801.113347	16.267725	-0.048390	3.765551
239.905487	4793.159700	16.272730	-0.048379	3.762573
239.782394	4785.133949	16.277735	-0.048351	3.759564
239.643451	4777.198077	16.282739	-0.048320	3.756586
239.650951	4769.136401	16.287744	-0.048317	3.753562
239.678011	4761.084999	16.292749	-0.048317	3.750540
239.493106	4753.129671	16.297754	-0.048277	3.747546
239.426494	4745.119466	16.302759	-0.048260	3.744532
239.660474	4737.179019	16.307763	-0.048298	3.741549
239.511821	4729.150356	16.312768	-0.048266	3.738521
239.552256	4721.192520	16.317773	-0.048268	3.735522
239.687142	4713.158171	16.322778	-0.048288	3.732494
239.423046	4705.133253	16.327783	-0.048234	3.729458
239.396002	4697.195720	16.332787	-0.048224	3.726457
239.509005	4689.155829	16.337792	-0.048240	3.723419
239.477498	4681.205897	16.342797	-0.048229	3.720409
239.166156	4673.258945	16.347802	-0.048167	3.717391
239.228742	4665.207287	16.352807	-0.048173	3.714340
239.297136	4657.135529	16.357811	-0.048181	3.711279
239.088029	4649.133562	16.362816	-0.048137	3.708235
238.921147	4641.156050	16.367821	-0.048101	3.705199
239.051586	4633.194513	16.372826	-0.048120	3.702174
239.025144	4625.197213	16.377831	-0.048110	3.699129
238.923926	4617.268747	16.382835	-0.048086	3.696105
238.797246	4609.227369	16.387840	-0.048058	3.693036
238.851384	4601.209448	16.392845	-0.048063	3.689977
238.863349	4593.249146	16.397850	-0.048060	3.686937
238.589620	4585.259646	16.402855	-0.048004	3.683876
238.606651	4577.289401	16.407859	-0.048002	3.680827
238.513572	4569.266269	16.412864	-0.047980	3.677752
238.625710	4561.256533	16.417869	-0.047996	3.674686
238.555379	4553.253467	16.422874	-0.047978	3.671614
238.365463	4545.232657	16.427879	-0.047937	3.668530
238.412586	4537.272553	16.432883	-0.047941	3.665473
238.307113	4529.272583	16.437888	-0.047917	3.662394
238.438943	4521.273031	16.442893	-0.047936	3.659319
238.365306	4513.308707	16.447898	-0.047918	3.656249
238.269388	4505.266010	16.452903	-0.047895	3.653147
238.216069	4497.267723	16.457907	-0.047880	3.650059
238.232486	4489.293270	16.462912	-0.047878	3.646980
238.245076	4481.289477	16.467917	-0.047875	3.643887
238.205436	4473.320284	16.472922	-0.047863	3.640804
238.307196	4465.296497	16.477927	-0.047877	3.637700
238.041992	4457.341211	16.482931	-0.047822	3.634611
237.861982	4449.289519	16.487936	-0.047784	3.631483
237.950656	4441.292039	16.492941	-0.047795	3.628382
237.960769	4433.292398	16.497946	-0.047792	3.625274
237.845817	4425.283505	16.502951	-0.047766	3.622157
237.693617	4417.325081	16.507955	-0.047733	3.619056
237.606201	4409.345747	16.512960	-0.047711	3.615946
237.561408	4401.336686	16.517965	-0.047698	3.612823
237.664720	4393.333673	16.522970	-0.047712	3.609703
237.661950	4385.354670	16.527975	-0.047707	3.606587
237.699138	4377.381316	16.532979	-0.047709	3.603472
237.448255	4369.376402	16.537984	-0.047657	3.600334
237.338943	4361.440176	16.542989	-0.047632	3.597224
237.280171	4353.435560	16.547994	-0.047616	3.594086
237.251812	4345.387238	16.552999	-0.047605	3.590928
237.293263	4337.408543	16.558003	-0.047608	3.587798
237.321641	4329.377380	16.563008	-0.047608	3.584643
237.305961	4321.426315	16.568013	-0.047600	3.581516
237.190313	4313.429227	16.573018	-0.047574	3.578365
237.188153	4305.425406	16.578023	-0.047569	3.575213
237.086561	4297.484214	16.583027	-0.047545	3.572079
236.981135	4289.433286	16.588032	-0.047520	3.568899
237.105627	4281.434289	16.593037	-0.047538	3.565743
236.880968	4273.474405	16.598042	-0.047491	3.562590
236.918872	4265.446250	16.603047	-0.047493	3.559414
236.865373	4257.514766	16.608051	-0.047478	3.556272
236.862840	4249.407819	16.613056	-0.047473	3.553058
236.823853	4241.349472	16.618061	-0.047461	3.549860
236.721243	4233.429690	16.623066	-0.047437	3.546712
236.540708	4225.423118	16.628071	-0.047398	3.543525
236.797158	4217.447474	16.633075	-0.047441	3.540359
236.490220	4209.507195	16.638080	-0.047379	3.537189
236.570255	4201.485436	16.643085	-0.047389	3.533994
236.717982	4193.442303	16.648090	-0.047411	3.530791
236.486200	4185.474303	16.653095	-0.047363	3.527602
236.476765	4177.475608	16.658099	-0.047356	3.524406
236.787849	4169.489366	16.663104	-0.047409	3.521221
236.533991	4161.526152	16.668109	-0.047357	3.518025
236.541743	4153.534653	16.673114	-0.047353	3.514823
236.562782	4145.497286	16.678119	-0.047352	3.511601
236.557064	4137.514441	16.683123	-0.047346	3.508396
236.340790	4129.524105	16.688128	-0.047301	3.505179
236.172068	4121.570888	16.693133	-0.047265	3.501975
236.200573	4113.570953	16.698138	-0.047265	3.498755
236.089818	4105.597735	16.703143	-0.047239	3.495539
236.083856	4097.609803	16.708147	-0.047233	3.492318
235.992500	4089.558625	16.713152	-0.047211	3.489065
236.283360	4081.586969	16.718157	-0.047260	3.485853
236.116920	4073.633027	16.723162	-0.047224	3.482631
235.907671	4065.626686	16.728167	-0.047180	3.479384
236.119385	4057.677837	16.733171	-0.047215	3.476170
235.882732	4049.619407	16.738176	-0.047166	3.472895
235.620763	4041.600685	16.743181	-0.047112	3.469631
235.642192	4033.646180	16.748186	-0.047111	3.466400
235.795989	4025.597984	16.753191	-0.047135	3.463132
235.600996	4017.680272	16.758195	-0.047093	3.459902
235.484072	4009.673416	16.763200	-0.047067	3.456636
235.575083	4001.644467	16.768205	-0.047078	3.453365
235.460242	3993.641203	16.773210	-0.047052	3.450094
235.359331	3985.655152	16.778215	-0.047028	3.446827
235.400663	3977.688097	16.783219	-0.047031	3.443570
235.198975	3969.699503	16.788224	-0.046989	3.440293
235.176428	3961.742122	16.793229	-0.046979	3.437031
235.251917	3953.724215	16.798234	-0.046988	3.433745
235.173223	3945.677912	16.803239	-0.046969	3.430439
235.245830	3937.697628	16.808243	-0.046977	3.427162
235.346796	3929.713516	16.813248	-0.046991	3.423881
235.226300	3921.724170	16.818253	-0.046964	3.420587
235.050369	3913.772138	16.823258	-0.046926	3.417304
235.122619	3905.766468	16.828263	-0.046934	3.414003
235.385112	3897.748206	16.833267	-0.046978	3.410701
235.208933	3889.784605	16.838272	-0.046940	3.407403
234.920226	3881.785378	16.843277	-0.046882	3.404084
235.069916	3873.832847	16.848282	-0.046905	3.400795
234.954986	3865.825022	16.853287	-0.046878	3.397472
234.985795	3857.818135	16.858291	-0.046879	3.394150
234.747040	3849.716275	16.863296	-0.046829	3.390777
234.787117	3841.733443	16.868301	-0.046832	3.387459
234.679275	3833.781403	16.873306	-0.046807	3.384145
234.642634	3825.823690	16.878311	-0.046795	3.380829
234.597210	3817.875300	16.883315	-0.046782	3.377513
234.573628	3809.861868	16.888320	-0.046772	3.374167
234.401389	3801.850397	16.893325	-0.046735	3.370813
234.477604	3793.864561	16.898330	-0.046744	3.367476
234.468086	3785.844757	16.903335	-0.046738	3.364118
234.372960	3777.942319	16.908339	-0.046715	3.360802
234.160012	3769.929918	16.913344	-0.046670	3.357434
234.432504	3761.884577	16.918349	-0.046716	3.354065
234.368396	3753.892595	16.923354	-0.046699	3.350703
234.100096	3745.908545	16.928359	-0.046644	3.347334
234.194868	3737.920428	16.933363	-0.046657	3.343973
233.994981	3729.948899	16.938368	-0.046615	3.340604
233.904498	3721.984847	16.943373	-0.046593	3.337240
233.962913	3713.972294	16.948378	-0.046599	3.333857
234.098036	3705.930147	16.953383	-0.046619	3.330461
233.877245	3697.987803	16.958387	-0.046573	3.327090
233.908834	3689.960005	16.963392	-0.046574	3.323689
233.998030	3682.008159	16.968397	-0.046585	3.320319
233.825476	3674.056596	16.973402	-0.046548	3.316936
233.603513	3666.030248	16.978407	-0.046502	3.313516
233.697425	3658.010683	16.983411	-0.046514	3.310107
233.681750	3650.013474	16.988416	-0.046506	3.306700
233.698225	3642.022386	16.993421	-0.046504	3.303294
233.696188	3634.050694	16.998426	-0.046499	3.299891
233.595963	3626.085788	17.003431	-0.046475	3.296484
233.452431	3618.106057	17.008435	-0.046444	3.293065
233.412025	3610.078779	17.013440	-0.046431	3.289627
233.369784	3602.111771	17.018445	-0.046418	3.286210
233.327614	3594.139247	17.023450	-0.046406	3.282788
233.120694	3586.118763	17.028455	-0.046362	3.279335
233.311920	3578.185415	17.033459	-0.046393	3.275931
233.330280	3570.134553	17.038464	-0.046391	3.272467
233.121346	3562.128103	17.043469	-0.046347	3.269009
233.186736	3554.158746	17.048474	-0.046354	3.265574
233.020644	3546.172649	17.053479	-0.046318	3.262119
232.831428	3538.221037	17.058483	-0.046278	3.258675
232.824285	3530.211459	17.063488	-0.046272	3.255209
233.148746	3522.190728	17.068493	-0.046327	3.251747
233.060111	3514.207819	17.073498	-0.046306	3.248282
232.864889	3506.190845	17.078503	-0.046264	3.244794
233.149831	3498.248730	17.083507	-0.046313	3.241355
232.988090	3490.276718	17.088512	-0.046277	3.237880
232.643374	3482.291657	17.093517	-0.046208	3.234389
232.844233	3474.218061	17.098522	-0.046241	3.230877
232.602372	3466.218054	17.103527	-0.046191	3.227376
232.663454	3458.244228	17.108531	-0.046197	3.223895
232.444741	3450.292366	17.113536	-0.046151	3.220408
232.264733	3442.314948	17.118541	-0.046113	3.216907
232.491205	3434.303787	17.123546	-0.046150	3.213405
232.414500	3426.295706	17.128551	-0.046131	3.209888
232.545772	3418.335748	17.133555	-0.046150	3.206396
232.407000	3410.358168	17.138560	-0.046119	3.202882
232.150787	3402.379295	17.143565	-0.046067	3.199359
232.148024	3394.450378	17.148570	-0.046061	3.195864
232.016046	3386.403135	17.153575	-0.046032	3.192308
232.195829	3378.393093	17.158579	-0.046060	3.188777
231.972017	3370.400802	17.163584	-0.046013	3.185233
232.002057	3362.426317	17.168589	-0.046014	3.181704
231.980755	3354.464893	17.173594	-0.046005	3.178175
231.899365	3346.455520	17.178599	-0.045985	3.174617
231.852711	3338.469380	17.183603	-0.045971	3.171068
231.847740	3330.467832	17.188608	-0.045965	3.167510
231.709531	3322.486776	17.193613	-0.045935	3.163951
231.586128	3314.542038	17.198618	-0.045907	3.160404
231.766523	3306.514521	17.203623	-0.045935	3.156830
231.905824	3298.520965	17.208627	-0.045956	3.153265
231.413300	3290.527560	17.213632	-0.045860	3.149669
231.418070	3282.542304	17.218637	-0.045855	3.146094
231.645100	3274.551315	17.223642	-0.045893	3.142522
231.391369	3266.589369	17.228647	-0.045841	3.138938
231.278189	3258.613101	17.233651	-0.045814	3.135350
231.304647	3250.606596	17.238656	-0.045814	3.131750
231.297485	3242.602212	17.243661	-0.045808	3.128145
231.058384	3234.666685	17.248666	-0.045759	3.124557
231.201667	3226.658252	17.253671	-0.045780	3.120949
231.193858	3218.689207	17.258675	-0.045774	3.117348
231.030323	3210.728317	17.263680	-0.045738	3.113739
231.081675	3202.667827	17.268685	-0.045743	3.110091
231.134423	3194.695076	17.273690	-0.045748	3.106478
230.885993	3186.692986	17.278695	-0.045697	3.102834
230.786994	3178.752030	17.283699	-0.045673	3.099220
230.873459	3170.779127	17.288704	-0.045684	3.095596
230.691393	3162.761048	17.293709	-0.045645	3.091935
230.790759	3154.777534	17.298714	-0.045659	3.088298
230.515508	3146.788619	17.303719	-0.045603	3.084637
230.869289	3138.789323	17.308723	-0.045663	3.080996
230.594610	3130.861688	17.313728	-0.045607	3.077355
230.601841	3122.831868	17.318733	-0.045604	3.073675
230.939537	3114.750134	17.323738	-0.045662	3.069983
230.415386	3106.833110	17.328743	-0.045559	3.066321
230.487302	3098.870317	17.333747	-0.045567	3.062662
230.698872	3090.872893	17.338752	-0.045602	3.058990
230.425620	3082.904250	17.343757	-0.045546	3.055303
230.282526	3074.919146	17.348762	-0.045514	3.051610
230.258113	3066.895781	17.353767	-0.045505	3.047901
230.462801	3058.911156	17.358771	-0.045538	3.044216
230.282484	3050.999460	17.363776	-0.045499	3.040542
230.220211	3043.007170	17.368781	-0.045483	3.036832
230.258692	3035.016243	17.373786	-0.045485	3.033123
229.988998	3026.996649	17.378791	-0.045430	3.029381
230.101352	3019.022380	17.383795	-0.045446	3.025674
229.973999	3011.046020	17.388800	-0.045417	3.021949
230.033481	3003.058027	17.393805	-0.045423	3.018224
229.948788	2995.108985	17.398810	-0.045402	3.014506
229.727421	2987.099442	17.403815	-0.045356	3.010747
229.854722	2979.121316	17.408819	-0.045375	3.007016
229.696792	2971.145809	17.413824	-0.045341	3.003268
229.737799	2963.136769	17.418829	-0.045343	2.999508
229.706494	2955.196483	17.423834	-0.045332	2.995773
229.697809	2947.155702	17.428839	-0.045326	2.991987
229.494915	2939.190047	17.433843	-0.045283	2.988222
229.438879	2931.212323	17.438848	-0.045268	2.984454
229.446036	2923.226095	17.443853	-0.045264	2.980680
229.438611	2915.259445	17.448858	-0.045258	2.976910
229.407326	2907.246176	17.453863	-0.045247	2.973112
229.462582	2899.252974	17.458867	-0.045252	2.969322
229.328879	2891.286924	17.463872	-0.045222	2.965532
229.208470	2883.325109	17.468877	-0.045195	2.961739
229.426513	2875.364654	17.473882	-0.045230	2.957959
229.254263	2867.371275	17.478887	-0.045193	2.954138
229.013039	2859.391201	17.483891	-0.045143	2.950316
229.226513	2851.373711	17.488896	-0.045178	2.946494
229.230891	2843.395691	17.493901	-0.045174	2.942675
229.053421	2835.449070	17.498906	-0.045136	2.938857
228.993843	2827.457794	17.503911	-0.045120	2.935018
228.893459	2819.463273	17.508915	-0.045096	2.931171
228.897832	2811.471758	17.513920	-0.045092	2.927326
228.734891	2803.505798	17.518925	-0.045057	2.923479
229.003833	2795.516683	17.523930	-0.045102	2.919638
228.844232	2787.577211	17.528935	-0.045067	2.915794
228.839141	2779.504904	17.533939	-0.045061	2.911889
228.512143	2771.517519	17.538944	-0.044995	2.908002
228.649479	2763.516782	17.543949	-0.045016	2.904129
228.626466	2755.587401	17.548954	-0.045007	2.900276
228.383273	2747.615963	17.553959	-0.044956	2.896386
228.487981	2739.648176	17.558963	-0.044971	2.892512
228.349144	2731.652168	17.563968	-0.044940	2.888605
228.286041	2723.657347	17.568973	-0.044923	2.884697
228.128439	2715.730500	17.573978	-0.044889	2.880813
228.125199	2707.736028	17.578983	-0.044883	2.876898
228.284892	2699.732305	17.583987	-0.044908	2.872982
228.181952	2691.734521	17.588992	-0.044884	2.869050
228.256473	2683.746242	17.593997	-0.044893	2.865126
228.291610	2675.804976	17.599002	-0.044894	2.861219
227.899372	2667.849265	17.604007	-0.044816	2.857275
228.031516	2659.864551	17.609011	-0.044836	2.853340
227.971111	2651.855112	17.614016	-0.044820	2.849377
227.746051	2643.905106	17.619021	-0.044773	2.845428
227.882745	2635.937821	17.624026	-0.044793	2.841486
227.989581	2627.930865	17.629031	-0.044808	2.837517
227.738834	2619.976993	17.634035	-0.044757	2.833549
227.277052	2612.002680	17.639040	-0.044666	2.829553
227.590912	2603.971982	17.644045	-0.044719	2.825567
227.676893	2596.002874	17.649050	-0.044730	2.821593
227.464515	2588.059777	17.654055	-0.044686	2.817610
227.489842	2580.069597	17.659059	-0.044685	2.813611
227.584482	2572.059151	17.664064	-0.044698	2.809600
227.386864	2564.112998	17.669069	-0.044656	2.805599
227.453418	2556.132933	17.674074	-0.044664	2.801590
227.453170	2548.151522	17.679079	-0.044659	2.797571
227.566202	2540.163523	17.684083	-0.044675	2.793550
227.206602	2532.201585	17.689088	-0.044603	2.789508
227.197808	2524.206957	17.694093	-0.044596	2.785464
227.199728	2516.265197	17.699098	-0.044592	2.781442
226.788722	2508.319665	17.704103	-0.044510	2.777388
226.715094	2500.338001	17.709107	-0.044491	2.773330
226.624160	2492.323475	17.714112	-0.044469	2.769247
226.562542	2484.353513	17.719117	-0.044453	2.765183
226.648856	2476.386515	17.724122	-0.044464	2.761124
226.577915	2468.400808	17.729127	-0.044446	2.757039
226.592111	2460.387084	17.734131	-0.044444	2.752939
226.579251	2452.364127	17.739136	-0.044436	2.748827
226.446389	2444.389833	17.744141	-0.044406	2.744726
226.646212	2436.447679	17.749146	-0.044439	2.740656
226.580118	2428.476579	17.754151	-0.044421	2.736549
226.571314	2420.499795	17.759155	-0.044415	2.732436
226.630284	2412.500992	17.764160	-0.044421	2.728310
226.246721	2404.574148	17.769165	-0.044344	2.724187
226.402584	2396.624144	17.774170	-0.044368	2.720079
226.194015	2388.670618	17.779175	-0.044325	2.715941
226.287900	2380.643925	17.784179	-0.044337	2.711777
226.273656	2372.656843	17.789184	-0.044329	2.707621
226.153365	2364.698941	17.794189	-0.044302	2.703467
226.071369	2356.742758	17.799194	-0.044282	2.699310
225.982781	2348.776393	17.804199	-0.044260	2.695140
225.949143	2340.791348	17.809203	-0.044249	2.690958
226.024834	2332.790660	17.814208	-0.044258	2.686768
225.725278	2324.859658	17.819213	-0.044197	2.682584
225.774573	2316.885310	17.824218	-0.044202	2.678393
225.926552	2308.892598	17.829223	-0.044225	2.674193
225.843533	2300.891829	17.834227	-0.044205	2.669966
225.731089	2292.929786	17.839232	-0.044179	2.665751
225.507486	2284.975084	17.844237	-0.044132	2.661527
225.576366	2277.011558	17.849242	-0.044140	2.657309
225.490477	2269.022565	17.854247	-0.044119	2.653062
225.289753	2261.073084	17.859251	-0.044077	2.648821
225.227595	2253.085487	17.864256	-0.044060	2.644562
225.258566	2245.129460	17.869261	-0.044061	2.640319
225.258524	2237.179216	17.874266	-0.044056	2.636071
225.052839	2229.172422	17.879271	-0.044013	2.631772
225.097873	2221.188033	17.884275	-0.044016	2.627494
224.997489	2213.246208	17.889280	-0.043992	2.623222
225.073231	2205.260773	17.894285	-0.044001	2.618932
225.096578	2197.304713	17.899290	-0.044001	2.614647
224.951177	2189.312693	17.904295	-0.043969	2.610324
224.808350	2181.363680	17.909299	-0.043937	2.606018
224.757693	2173.405747	17.914304	-0.043923	2.601706
224.721312	2165.433657	17.919309	-0.043911	2.597379
224.789614	2157.388289	17.924314	-0.043919	2.593013
224.662853	2149.302596	17.929319	-0.043890	2.588605
224.615668	2141.355821	17.934323	-0.043876	2.584270
224.562372	2133.456020	17.939328	-0.043861	2.579952
224.602913	2125.497785	17.944333	-0.043864	2.575603
224.521655	2117.555493	17.949338	-0.043844	2.571246
224.355301	2109.584008	17.954343	-0.043808	2.566859
224.319033	2101.639603	17.959347	-0.043796	2.562489
224.421176	2093.671147	17.964352	-0.043810	2.558109
224.506120	2085.683961	17.969357	-0.043821	2.553709
224.550799	2077.718415	17.974362	-0.043825	2.549310
224.191581	2069.759867	17.979367	-0.043753	2.544880
224.053326	2061.844365	17.984371	-0.043722	2.540481
224.076585	2053.876297	17.989376	-0.043721	2.536056
224.128188	2045.863841	17.994381	-0.043726	2.531601
224.199043	2037.897403	17.999386	-0.043734	2.527166
223.745642	2029.983538	18.004391	-0.043645	2.522714
223.866245	2022.010587	18.009395	-0.043662	2.518263
223.824188	2014.050833	18.014400	-0.043649	2.513800
223.759148	2006.025682	18.019405	-0.043632	2.509290
223.764851	1998.065779	18.024410	-0.043628	2.504813
223.522559	1990.121360	18.029415	-0.043578	2.500320
223.713126	1982.144007	18.034419	-0.043609	2.495831
223.624789	1974.180835	18.039424	-0.043587	2.491322
223.374692	1966.235743	18.044429	-0.043536	2.486803
223.521020	1958.277980	18.049434	-0.043558	2.482298
223.387939	1950.328909	18.054439	-0.043528	2.477769
223.316093	1942.362108	18.059443	-0.043510	2.473226
223.418228	1934.358607	18.064448	-0.043524	2.468667
223.487925	1926.371054	18.069453	-0.043532	2.464105
223.492993	1918.442903	18.074458	-0.043528	2.459565
223.233288	1910.511046	18.079463	-0.043475	2.454994
223.087221	1902.544493	18.084467	-0.043443	2.450404
223.092944	1894.578979	18.089472	-0.043439	2.445816
222.824082	1886.658289	18.094477	-0.043384	2.441225
223.028267	1878.697376	18.099482	-0.043417	2.436639
222.939041	1870.651354	18.104487	-0.043395	2.431971
222.713702	1862.698728	18.109491	-0.043348	2.427339
222.613769	1854.747513	18.114496	-0.043325	2.422708
222.656309	1846.779565	18.119501	-0.043328	2.418070
222.634608	1838.834857	18.124506	-0.043319	2.413431
222.515703	1830.854877	18.129511	-0.043291	2.408755
222.533282	1822.892794	18.134515	-0.043290	2.404091
222.503595	1814.969174	18.139520	-0.043279	2.399437
222.294570	1807.026010	18.144525	-0.043235	2.394748
222.318122	1799.048930	18.149530	-0.043235	2.390048
222.308999	1791.073403	18.154535	-0.043228	2.385338
222.363486	1783.120389	18.159539	-0.043233	2.380636
222.503467	1775.149736	18.164544	-0.043254	2.375921
222.324354	1767.200935	18.169549	-0.043216	2.371185
222.271430	1759.262143	18.174554	-0.043201	2.366455
221.969199	1751.339381	18.179559	-0.043140	2.361705
221.974817	1743.381281	18.184563	-0.043136	2.356950
221.940755	1735.397982	18.189568	-0.043125	2.352166
221.759228	1727.420230	18.194573	-0.043086	2.347364
221.948607	1719.460764	18.199578	-0.043116	2.342593
221.851502	1711.524947	18.204583	-0.043093	2.337803
221.609417	1703.588737	18.209587	-0.043043	2.332992
221.749701	1695.606177	18.214592	-0.043064	2.328174
221.772582	1687.626205	18.219597	-0.043064	2.323337
221.889975	1679.702022	18.224602	-0.043081	2.318533
221.799406	1671.747557	18.229607	-0.043059	2.313682
221.631331	1663.796405	18.234611	-0.043022	2.308817
221.486321	1655.857420	18.239616	-0.042991	2.303951
221.419534	1647.912338	18.244621	-0.042973	2.299078
221.295683	1639.983345	18.249626	-0.042945	2.294199
221.264049	1631.987129	18.254631	-0.042934	2.289276
221.288975	1624.044072	18.259635	-0.042934	2.284381
221.132399	1616.130955	18.264640	-0.042900	2.279477
220.967898	1608.199292	18.269645	-0.042864	2.274551
221.283687	1600.103863	18.274650	-0.042918	2.269554
221.003742	1592.183815	18.279655	-0.042861	2.264604
221.166223	1584.236860	18.284659	-0.042886	2.259664
220.922920	1576.341597	18.289664	-0.042836	2.254710
220.707508	1568.389479	18.294669	-0.042791	2.249713
220.714146	1560.431918	18.299674	-0.042787	2.244720
220.781724	1552.481306	18.304679	-0.042795	2.239726
220.778879	1544.560929	18.309683	-0.042789	2.234733
220.915953	1536.552516	18.314688	-0.042810	2.229686
220.783037	1528.615971	18.319693	-0.042780	2.224649
220.707733	1520.709048	18.324698	-0.042761	2.219625
220.585788	1512.774405	18.329703	-0.042734	2.214567
220.543624	1504.807843	18.334707	-0.042721	2.209485
220.470843	1496.876140	18.339712	-0.042702	2.204410
220.247709	1488.967156	18.344717	-0.042656	2.199325
220.288002	1481.019951	18.349722	-0.042658	2.194227
220.225261	1473.019000	18.354727	-0.042642	2.189073
220.133699	1465.078956	18.359731	-0.042620	2.183944
220.029367	1457.164490	18.364736	-0.042595	2.178817
219.893717	1449.230810	18.369741	-0.042565	2.173664
219.773233	1441.290584	18.374746	-0.042538	2.168495
219.777905	1433.333329	18.379751	-0.042534	2.163315
219.958236	1425.383672	18.384755	-0.042562	2.158143
219.785513	1417.473325	18.389760	-0.042525	2.152952
219.740705	1409.491121	18.394765	-0.042512	2.147713
219.642097	1401.580460	18.399770	-0.042488	2.142503
219.622796	1393.638685	18.404775	-0.042480	2.137268
219.641924	1385.683000	18.409779	-0.042478	2.132014
219.541975	1377.766368	18.414784	-0.042455	2.126761
219.434232	1369.838534	18.419789	-0.042430	2.121487
219.496335	1361.910200	18.424794	-0.042437	2.116216
219.375548	1353.906457	18.429799	-0.042409	2.110864
219.176340	1345.973107	18.434803	-0.042367	2.105538
219.265297	1338.044513	18.439808	-0.042379	2.100230
219.186730	1330.119117	18.444813	-0.042359	2.094894
219.005156	1322.199992	18.449818	-0.042320	2.089538
218.902258	1314.264936	18.454823	-0.042296	2.084166
218.940328	1306.346678	18.459827	-0.042298	2.078804
218.890153	1298.430902	18.464832	-0.042284	2.073422
218.763849	1290.468976	18.469837	-0.042256	2.067987
218.855436	1282.530008	18.474842	-0.042268	2.062575
218.747271	1274.618009	18.479847	-0.042243	2.057148
218.464921	1266.711135	18.484851	-0.042185	2.051691
218.502564	1258.757490	18.489856	-0.042187	2.046221
218.535069	1250.819718	18.494861	-0.042188	2.040746
218.509306	1242.920326	18.499866	-0.042178	2.035277
218.333264	1234.962518	18.504871	-0.042141	2.029737
218.441849	1227.024685	18.509875	-0.042156	2.024225
218.322747	1219.123654	18.514880	-0.042129	2.018701
217.998626	1211.227389	18.519885	-0.042064	2.013143
218.105514	1203.265585	18.524890	-0.042079	2.007569
217.921888	1195.363744	18.529895	-0.042039	2.001991
217.841905	1187.461371	18.534899	-0.042020	1.996408
218.006866	1179.486793	18.539904	-0.042045	1.990784
218.050672	1171.538993	18.544909	-0.042049	1.985150
217.945971	1163.655095	18.549914	-0.042024	1.979530
217.914423	1155.739254	18.554919	-0.042013	1.973879
217.784944	1147.816484	18.559923	-0.041984	1.968196
217.803755	1139.899056	18.564928	-0.041983	1.962516
217.654350	1132.003051	18.569933	-0.041950	1.956818
217.534844	1124.060010	18.574938	-0.041923	1.951071
217.405233	1116.107719	18.579943	-0.041894	1.945300
217.490389	1108.187177	18.584947	-0.041905	1.939559
217.350426	1100.302893	18.589952	-0.041874	1.933802
217.229366	1092.362503	18.594957	-0.041846	1.927989
217.205777	1084.470780	18.599962	-0.041837	1.922204
216.975308	1076.583997	18.604967	-0.041789	1.916383
217.147892	1068.624844	18.609971	-0.041816	1.910536
217.064020	1060.718180	18.614976	-0.041796	1.904681
216.902655	1052.833326	18.619981	-0.041761	1.898815
217.034541	1044.915003	18.624986	-0.041780	1.892939
216.810612	1037.001072	18.629991	-0.041734	1.887008
216.619398	1029.126561	18.634995	-0.041693	1.881091
216.745775	1021.210491	18.640000	-0.041712	1.875161
216.696737	1013.269129	18.645005	-0.041698	1.869173
216.715864	1005.358684	18.650010	-0.041696	1.863196
216.434191	997.482996	18.655015	-0.041639	1.857192
216.396513	989.567131	18.660019	-0.041627	1.851167
216.494272	981.646052	18.665024	-0.041640	1.845133
216.329300	973.774004	18.670029	-0.041605	1.839086
216.473374	965.868871	18.675034	-0.041626	1.833031
216.439922	957.950701	18.680039	-0.041615	1.826924
216.196751	950.085274	18.685043	-0.041565	1.820812
216.133638	942.198157	18.690048	-0.041548	1.814685
215.850318	934.306469	18.695053	-0.041491	1.808507
215.962381	926.400540	18.700058	-0.041507	1.802344
215.789652	918.529044	18.705063	-0.041470	1.796152
215.819710	910.564409	18.710067	-0.041470	1.789891
215.806009	902.669304	18.715072	-0.041463	1.783657
215.552217	894.806834	18.720077	-0.041411	1.777397
215.687167	886.896449	18.725082	-0.041431	1.771125
215.521985	879.016937	18.730087	-0.041395	1.764819
215.549171	871.139376	18.735091	-0.041395	1.758515
215.440414	863.276710	18.740096	-0.041370	1.752183
215.297965	855.384222	18.745101	-0.041339	1.745800
215.327967	847.502914	18.750106	-0.041339	1.739425
215.346728	839.614784	18.755111	-0.041338	1.733019
215.105218	831.746166	18.760115	-0.041288	1.726572
215.180804	823.865270	18.765120	-0.041297	1.720131
214.986602	816.013549	18.770125	-0.041256	1.713656
215.034960	808.105059	18.775130	-0.041260	1.707140
215.074551	800.208466	18.780135	-0.041263	1.700608
214.915484	792.363370	18.785139	-0.041228	1.694068
214.957412	784.472998	18.790144	-0.041231	1.687491
214.829210	776.619575	18.795149	-0.041202	1.680897
214.806687	768.767502	18.800154	-0.041193	1.674292
214.604897	760.905436	18.805159	-0.041151	1.667628
214.588950	753.030702	18.810163	-0.041143	1.660952
214.521292	745.177320	18.815168	-0.041125	1.654260
214.203890	737.333693	18.820173	-0.041061	1.647515
214.280898	729.469357	18.825178	-0.041071	1.640778
214.219493	721.607195	18.830183	-0.041054	1.633997
214.018919	713.719784	18.835187	-0.041012	1.627146
213.817190	705.889047	18.840192	-0.040970	1.620315
213.731233	698.031502	18.845197	-0.040949	1.613448
213.771564	690.155702	18.850202	-0.040951	1.606553
213.532122	682.336578	18.855207	-0.040902	1.599639
213.448482	674.502068	18.860211	-0.040881	1.592704
213.476595	666.629135	18.865216	-0.040882	1.585720
213.330161	658.797424	18.870221	-0.040850	1.578716
213.319694	650.951301	18.875226	-0.040843	1.571689
213.558349	643.052343	18.880231	-0.040882	1.564618
213.605518	635.228853	18.885235	-0.040886	1.557555
213.486915	627.402359	18.890240	-0.040859	1.550434
213.273410	619.582859	18.895245	-0.040815	1.543271
213.104875	611.781977	18.900250	-0.040778	1.536099
212.917695	603.952311	18.905255	-0.040739	1.528864
212.687984	596.148569	18.910259	-0.040691	1.521612
213.069480	588.273435	18.915264	-0.040757	1.514352
212.782140	580.471391	18.920269	-0.040699	1.507023
212.688653	572.669589	18.925274	-0.040676	1.499688
212.668875	564.841576	18.930279	-0.040668	1.492303
212.545398	557.030098	18.935283	-0.040640	1.484882
212.340039	549.267212	18.940288	-0.040597	1.477456
212.260650	541.404747	18.945293	-0.040577	1.469918
212.477817	533.544755	18.950298	-0.040613	1.462389
212.279396	525.771773	18.955303	-0.040571	1.454840
212.109332	517.980957	18.960307	-0.040534	1.447239
212.204231	510.173656	18.965312	-0.040547	1.439624
211.959055	502.409497	18.970317	-0.040497	1.431956
211.938142	494.606274	18.975322	-0.040488	1.424245
211.795049	486.838149	18.980327	-0.040456	1.416506
211.836639	479.029127	18.985331	-0.040459	1.408714
212.045604	471.222066	18.990336	-0.040493	1.400909
211.722787	463.492233	18.995341	-0.040428	1.393049
211.784660	455.685567	19.000346	-0.040435	1.385132
211.461311	447.961776	19.005351	-0.040370	1.377188
211.229777	440.207266	19.010355	-0.040322	1.369182
211.306229	432.423166	19.015360	-0.040332	1.361151
211.343368	424.650896	19.020365	-0.040334	1.353078
211.417578	416.878742	19.025370	-0.040343	1.344963
211.285209	409.141563	19.030375	-0.040313	1.336800
211.033852	401.418014	19.035379	-0.040261	1.328580
210.973758	393.686384	19.040384	-0.040245	1.320334
211.020866	385.872998	19.045389	-0.040249	1.311967
211.060767	378.060165	19.050394	-0.040252	1.303546
210.870881	370.363885	19.055399	-0.040212	1.295155
210.645165	362.664893	19.060403	-0.040165	1.286700
210.734346	354.945429	19.065408	-0.040177	1.278225
210.243317	347.295784	19.070413	-0.040081	1.269662
210.307080	339.562885	19.075418	-0.040088	1.261052
210.305926	331.855450	19.080423	-0.040083	1.252400
210.249946	324.153675	19.085427	-0.040067	1.243683
210.044559	316.499813	19.090432	-0.040024	1.234931
209.851973	308.803675	19.095437	-0.039984	1.226069
210.038335	301.088687	19.100442	-0.040014	1.217196
209.604850	293.469113	19.105447	-0.039928	1.208246
209.453466	285.812893	19.110451	-0.039895	1.199243
209.466609	278.137374	19.115456	-0.039893	1.190182
209.425522	270.461941	19.120461	-0.039880	1.181040
209.350850	262.831081	19.125466	-0.039862	1.171873
209.287543	255.179143	19.130471	-0.039845	1.162612
209.410150	247.512776	19.135475	-0.039863	1.153297
209.310871	239.868868	19.140480	-0.039840	1.143886
208.865704	232.308548	19.145485	-0.039752	1.134429
209.069428	224.647762	19.150490	-0.039786	1.124905
208.782773	217.091480	19.155495	-0.039727	1.115325
208.764791	209.476392	19.160499	-0.039719	1.105646
208.785346	201.887797	19.165504	-0.039718	1.095924
208.538824	194.328475	19.170509	-0.039668	1.086094
208.451784	186.780752	19.175514	-0.039647	1.076225
208.426558	179.199405	19.180519	-0.039637	1.066234
208.222605	171.678425	19.185523	-0.039595	1.056188
208.165997	164.129650	19.190528	-0.039580	1.046042
207.934663	156.639735	19.195533	-0.039532	1.035836
207.914460	149.112847	19.200538	-0.039523	1.025528
207.929636	141.597752	19.205543	-0.039522	1.015139
207.636328	134.142137	19.210547	-0.039462	1.004652
207.652128	126.650904	19.215552	-0.039461	0.994080
207.385282	119.175963	19.220557	-0.039406	0.983346
207.124984	111.761351	19.225562	-0.039353	0.972584
207.222672	104.283607	19.230567	-0.039367	0.961699
207.091645	96.874123	19.235571	-0.039338	0.950733
206.737803	89.512865	19.240576	-0.039267	0.939652
206.485520	82.139933	19.245581	-0.039216	0.928447
206.562295	74.746483	19.250586	-0.039225	0.917163
206.230881	67.414370	19.255591	-0.039159	0.905723
206.094414	60.309262	19.260595	-0.039129	0.894548