Fri Mar 12 12:38:07 2021

Number of Points = 3621
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.877103	-0.116245	0.000000	-0.000073	0.728488

0.636814	-0.115474	0.005005	-0.000029	0.728407
0.715444	-0.123904	0.010010	-0.000044	0.728419
0.798648	-0.141529	0.015014	-0.000060	0.728414
0.621228	-0.112165	0.020019	-0.000027	0.728410
0.754174	-0.132067	0.025024	-0.000052	0.728418
0.580018	-0.107415	0.030029	-0.000020	0.728407
0.577653	-0.102753	0.035034	-0.000020	0.728416
0.695958	-0.125662	0.040038	-0.000043	0.728413
0.921168	-0.167679	0.045043	-0.000085	0.728410
0.710888	-0.127255	0.050048	-0.000046	0.728417
0.569977	-0.109001	0.055053	-0.000020	0.728404
0.706314	-0.129145	0.060058	-0.000046	0.728413
0.878665	-0.162797	0.065062	-0.000079	0.728408
0.899150	-0.326336	0.070067	-0.000083	0.728098
0.600062	-0.280447	0.075072	-0.000028	0.728084
0.484849	-0.264079	0.080077	-0.000007	0.728077
0.635805	-0.286387	0.085082	-0.000035	0.728087
0.588950	-0.282225	0.090086	-0.000027	0.728079
0.521913	-0.271705	0.095091	-0.000015	0.728077
0.731430	-0.348444	0.100096	-0.000054	0.728001
0.723555	-0.468827	0.105101	-0.000053	0.727765
0.770125	-0.473479	0.110106	-0.000062	0.727773
0.520492	-0.432862	0.115110	-0.000016	0.727766
0.617972	-0.452746	0.120115	-0.000035	0.727762
0.475125	-0.466070	0.125120	-0.000009	0.727687
0.266486	-0.553749	0.130125	0.000030	0.727445
0.558438	-0.601159	0.135130	-0.000025	0.727455
0.492179	-0.591978	0.140134	-0.000013	0.727450
0.623241	-0.618239	0.145139	-0.000038	0.727445
0.660770	-0.753216	0.150144	-0.000045	0.727196
0.263369	-0.708951	0.155149	0.000028	0.727145
0.240807	-0.700301	0.160154	0.000032	0.727155
0.432608	-0.736172	0.165158	-0.000004	0.727152
0.230356	-0.856067	0.170163	0.000033	0.726849
0.144913	-0.849751	0.175168	0.000049	0.726833
-0.003843	-0.828003	0.180173	0.000076	0.726824
0.338936	-0.929479	0.185178	0.000012	0.726746
0.183152	-1.018043	0.190182	0.000041	0.726520
-0.325401	-0.928289	0.195187	0.000135	0.726519
-0.372991	-0.916148	0.200192	0.000143	0.726527
-0.006464	-1.098850	0.205197	0.000075	0.726299
0.058105	-1.153413	0.210202	0.000062	0.726216
0.008755	-1.147597	0.215206	0.000071	0.726211
0.195541	-1.265282	0.220211	0.000036	0.726047
0.238345	-1.329145	0.225216	0.000028	0.725937
0.043337	-1.299277	0.230221	0.000063	0.725929
0.152618	-1.442045	0.235226	0.000043	0.725689
0.063103	-1.470902	0.240230	0.000059	0.725602
-0.129010	-1.442146	0.245235	0.000094	0.725592
-0.342692	-1.556951	0.250240	0.000134	0.725294
-0.239601	-1.579107	0.255245	0.000114	0.725288
-0.430289	-1.589568	0.260250	0.000149	0.725202
-1.356654	-1.543653	0.265254	0.000321	0.724970
-2.018063	-1.432822	0.270259	0.000444	0.724957
-1.877183	-1.457793	0.275264	0.000417	0.724958
-2.260646	-1.545821	0.280269	0.000488	0.724653
-2.723084	-1.468053	0.285274	0.000574	0.724645
-2.407834	-1.525105	0.290278	0.000515	0.724644
-2.209391	-1.640694	0.295283	0.000478	0.724488
-3.545207	-1.498191	0.300288	0.000726	0.724302
-3.771680	-1.468050	0.305293	0.000767	0.724283
-3.504987	-1.508006	0.310298	0.000717	0.724298
-3.551155	-1.569045	0.315302	0.000726	0.724164
-4.781058	-1.451683	0.320307	0.000954	0.723965
-4.463215	-1.505931	0.325312	0.000895	0.723971
-4.672542	-1.475529	0.330317	0.000933	0.723958
-4.821789	-1.443669	0.335322	0.000960	0.723969
-4.830084	-1.546836	0.340326	0.000962	0.723765
-5.871568	-1.431571	0.345331	0.001155	0.723628
-5.774723	-1.445798	0.350336	0.001137	0.723635
-5.962384	-1.417258	0.355341	0.001171	0.723626
-5.508738	-1.493297	0.360346	0.001086	0.723636
-5.538098	-1.509112	0.365350	0.001091	0.723596
-6.759160	-1.425044	0.370355	0.001318	0.723336
-6.470263	-1.475417	0.375360	0.001264	0.723338
-6.625235	-1.452655	0.380365	0.001292	0.723330
-6.771051	-1.423082	0.385370	0.001319	0.723338
-6.768482	-1.423989	0.390374	0.001318	0.723338
-6.703147	-1.438301	0.395379	0.001306	0.723333
-6.834648	-1.577542	0.400384	0.001330	0.723015
-7.822799	-1.413434	0.405389	0.001513	0.722993
-7.899599	-1.395076	0.410394	0.001527	0.723003
-7.468260	-1.473241	0.415398	0.001446	0.723001
-7.971649	-1.386012	0.420403	0.001540	0.722997
-7.788525	-1.416680	0.425408	0.001505	0.723001
-7.580281	-1.511427	0.430413	0.001466	0.722889
-8.510605	-1.448790	0.435418	0.001639	0.722688
-8.376055	-1.473913	0.440422	0.001613	0.722686
-8.670411	-1.424378	0.445427	0.001668	0.722681
-8.548094	-1.441555	0.450432	0.001644	0.722691
-8.674421	-1.423410	0.455437	0.001667	0.722684
-8.505053	-1.451670	0.460442	0.001635	0.722688
-8.428268	-1.576671	0.465446	0.001621	0.722470
-9.849256	-1.378696	0.470451	0.001885	0.722363
-9.443107	-1.446256	0.475456	0.001809	0.722373
-9.153608	-1.501155	0.480461	0.001755	0.722368
-9.645822	-1.412492	0.485466	0.001846	0.722370
-9.811150	-1.385691	0.490470	0.001876	0.722366
-9.605386	-1.425084	0.495475	0.001837	0.722361
-9.337848	-1.565954	0.500480	0.001787	0.722179
-10.778329	-1.365592	0.505485	0.002055	0.722070
-10.347558	-1.439288	0.510490	0.001974	0.722076
-10.144735	-1.477641	0.515494	0.001936	0.722073
-10.942435	-1.339390	0.520499	0.002084	0.722066
-10.494841	-1.414492	0.525504	0.002000	0.722076
-10.186748	-1.473815	0.530509	0.001943	0.722068
-10.524464	-1.506872	0.535514	0.002005	0.721886
-11.514859	-1.402634	0.540518	0.002189	0.721745
-11.522571	-1.404729	0.545523	0.002190	0.721739
-11.367977	-1.427861	0.550528	0.002161	0.721748
-11.924524	-1.333777	0.555533	0.002264	0.721739
-11.460158	-1.415643	0.560538	0.002177	0.721742
-11.349162	-1.435778	0.565542	0.002156	0.721742
-11.914083	-1.339925	0.570547	0.002261	0.721733
-11.607810	-1.496901	0.575552	0.002203	0.721533
-12.594386	-1.373728	0.580557	0.002387	0.721430
-12.455508	-1.395056	0.585562	0.002360	0.721438
-12.354173	-1.414781	0.590566	0.002341	0.721435
-12.684729	-1.358513	0.595571	0.002402	0.721431
-11.913658	-1.491344	0.600576	0.002258	0.721441
-12.659105	-1.363420	0.605581	0.002396	0.721432
-12.389658	-1.451949	0.610586	0.002346	0.721353
-12.920670	-1.476124	0.615590	0.002444	0.721120
-13.229118	-1.424465	0.620595	0.002501	0.721115
-13.250860	-1.416241	0.625600	0.002505	0.721124
-13.336843	-1.405388	0.630605	0.002521	0.721116
-12.980787	-1.466742	0.635610	0.002454	0.721121
-13.307883	-1.410016	0.640614	0.002514	0.721119
-13.385186	-1.420312	0.645619	0.002528	0.721072
-13.651579	-1.471486	0.650624	0.002577	0.720879
-14.197447	-1.380323	0.655629	0.002679	0.720868
-14.132718	-1.389801	0.660634	0.002666	0.720873
-13.528016	-1.496585	0.665638	0.002553	0.720876
-14.102165	-1.396895	0.670643	0.002660	0.720871
-14.178201	-1.380710	0.675648	0.002673	0.720877
-14.068893	-1.452670	0.680653	0.002653	0.720775
-14.982068	-1.412136	0.685658	0.002822	0.720535
-14.916677	-1.423636	0.690662	0.002810	0.720537
-15.133696	-1.389008	0.695667	0.002850	0.720529
-14.755080	-1.453234	0.700672	0.002779	0.720537
-15.089425	-1.398584	0.705677	0.002840	0.720528
-15.153799	-1.383486	0.710682	0.002852	0.720536
-14.876548	-1.455077	0.715686	0.002800	0.720493
-15.516078	-1.480938	0.720691	0.002919	0.720218
-15.797001	-1.427674	0.725696	0.002970	0.720226
-16.164940	-1.367197	0.730701	0.003039	0.720216
-15.677448	-1.452639	0.735706	0.002947	0.720220
-15.875424	-1.417713	0.740710	0.002984	0.720220
-16.185440	-1.365530	0.745715	0.003041	0.720215
-15.547006	-1.491129	0.750720	0.002922	0.720192
-16.594774	-1.458368	0.755725	0.003116	0.719890
-17.049772	-1.373866	0.760730	0.003201	0.719898
-16.708499	-1.434380	0.765734	0.003137	0.719899
-16.722728	-1.434633	0.770739	0.003139	0.719894
-16.693745	-1.435332	0.775744	0.003133	0.719904
-16.774884	-1.426482	0.780749	0.003148	0.719894
-16.457529	-1.481309	0.785754	0.003088	0.719898
-17.269538	-1.480328	0.790758	0.003239	0.719616
-17.846143	-1.387474	0.795763	0.003346	0.719597
-17.236168	-1.492279	0.800768	0.003232	0.719605
-17.580750	-1.436034	0.805773	0.003296	0.719596
-18.196204	-1.324896	0.810778	0.003410	0.719600
-17.564645	-1.436515	0.815782	0.003292	0.719602
-17.550709	-1.444753	0.820787	0.003289	0.719592
-18.217197	-1.461387	0.825792	0.003413	0.719326
-19.019759	-1.349578	0.830797	0.003562	0.719265
-18.645844	-1.415275	0.835802	0.003492	0.719268
-18.348737	-1.467610	0.840806	0.003436	0.719270
-19.082508	-1.342008	0.845811	0.003572	0.719261
-18.500894	-1.440975	0.850816	0.003463	0.719271
-18.743913	-1.401825	0.855821	0.003508	0.719263
-19.038423	-1.356829	0.860826	0.003562	0.719249
-19.222162	-1.471356	0.865830	0.003596	0.718960
-19.333106	-1.454777	0.870835	0.003616	0.718954
-19.892396	-1.349762	0.875840	0.003720	0.718966
-19.824795	-1.367790	0.880845	0.003707	0.718955
-19.505258	-1.423923	0.885850	0.003647	0.718957
-19.695775	-1.388859	0.890854	0.003682	0.718960
-19.892830	-1.357220	0.895859	0.003719	0.718954
-19.646606	-1.471419	0.900864	0.003672	0.718816
-20.509693	-1.408239	0.905869	0.003833	0.718638
-20.628852	-1.384579	0.910874	0.003854	0.718644
-20.453524	-1.415544	0.915878	0.003821	0.718645
-20.444060	-1.422266	0.920883	0.003819	0.718636
-20.425731	-1.421591	0.925888	0.003815	0.718645
-20.910407	-1.340503	0.930893	0.003905	0.718635
-20.738272	-1.380903	0.935898	0.003873	0.718617
-20.953190	-1.477487	0.940902	0.003912	0.718351
-21.329534	-1.414702	0.945907	0.003982	0.718344
-21.420830	-1.393199	0.950912	0.003998	0.718355
-21.201814	-1.437756	0.955917	0.003957	0.718345
-21.549165	-1.374482	0.960922	0.004021	0.718348
-21.741539	-1.339285	0.965926	0.004057	0.718351
-21.431691	-1.398637	0.970931	0.003999	0.718344
-21.675584	-1.503006	0.975936	0.004044	0.718052
-22.705501	-1.341902	0.980941	0.004235	0.718009
-22.537335	-1.370763	0.985946	0.004203	0.718012
-21.952552	-1.474106	0.990950	0.004094	0.718014
-22.851296	-1.317204	0.995955	0.004261	0.718009
-22.616841	-1.355739	1.000960	0.004217	0.718016
-22.221520	-1.431222	1.005965	0.004143	0.718007
-22.564330	-1.434133	1.010970	0.004206	0.717881
-23.643310	-1.333866	1.015974	0.004407	0.717701
-23.356330	-1.389499	1.020979	0.004353	0.717692
-23.338691	-1.389181	1.025984	0.004349	0.717700
-23.746506	-1.318611	1.030989	0.004424	0.717697
-23.580305	-1.348585	1.035994	0.004393	0.717697
-23.163329	-1.422002	1.040998	0.004315	0.717699
-23.617151	-1.346120	1.046003	0.004399	0.717690
-23.630842	-1.421557	1.051008	0.004401	0.717537
-24.636439	-1.328114	1.056013	0.004588	0.717369
-24.339188	-1.379576	1.061018	0.004532	0.717372
-24.286292	-1.389605	1.066022	0.004522	0.717372
-24.628288	-1.331112	1.071027	0.004585	0.717368
-24.270309	-1.390036	1.076032	0.004518	0.717378
-24.640387	-1.328436	1.081037	0.004587	0.717371
-24.588893	-1.336479	1.086042	0.004577	0.717374
-24.404856	-1.455741	1.091046	0.004542	0.717204
-25.637417	-1.301232	1.096051	0.004771	0.717076
-25.416094	-1.338146	1.101056	0.004729	0.717081
-25.027577	-1.412060	1.106061	0.004657	0.717073
-25.231370	-1.373330	1.111066	0.004694	0.717079
-25.187551	-1.380835	1.116070	0.004686	0.717080
-25.260704	-1.370622	1.121075	0.004699	0.717075
-24.968648	-1.486053	1.126080	0.004644	0.716951
-26.393827	-1.336758	1.131085	0.004909	0.716744
-26.012965	-1.402842	1.136090	0.004838	0.716749
-25.997976	-1.403320	1.141094	0.004834	0.716754
-26.347068	-1.344859	1.146099	0.004899	0.716747
-25.815353	-1.435172	1.151104	0.004799	0.716757
-26.012162	-1.405218	1.156109	0.004836	0.716748
-26.138317	-1.443957	1.161114	0.004859	0.716627
-27.037216	-1.375544	1.166118	0.005026	0.716446
-26.986841	-1.387766	1.171123	0.005016	0.716441
-26.891875	-1.400323	1.176128	0.004998	0.716450
-27.058048	-1.375192	1.181133	0.005028	0.716442
-26.912064	-1.401095	1.186138	0.005001	0.716443
-26.672099	-1.442792	1.191142	0.004956	0.716446
-27.152262	-1.425576	1.196147	0.005045	0.716312
-28.148076	-1.339026	1.201152	0.005229	0.716133
-27.646654	-1.432697	1.206157	0.005136	0.716125
-27.646098	-1.432695	1.211162	0.005135	0.716126
-27.756493	-1.411076	1.216166	0.005155	0.716130
-27.956606	-1.379463	1.221171	0.005192	0.716123
-27.726236	-1.416932	1.226176	0.005149	0.716131
-28.100522	-1.388133	1.231181	0.005218	0.716057
-28.661451	-1.379212	1.236186	0.005322	0.715877
-28.271205	-1.447447	1.241190	0.005249	0.715881
-28.803649	-1.357301	1.246195	0.005348	0.715872
-28.696549	-1.372104	1.251200	0.005327	0.715882
-28.557812	-1.399631	1.256205	0.005301	0.715877
-28.767521	-1.361384	1.261210	0.005340	0.715879
-28.714058	-1.446374	1.266214	0.005329	0.715731
-29.826084	-1.346280	1.271219	0.005536	0.715537
-29.225916	-1.448410	1.276224	0.005424	0.715547
-29.635314	-1.376834	1.281229	0.005500	0.715546
-30.079440	-1.299032	1.286234	0.005582	0.715544
-29.309470	-1.434245	1.291238	0.005438	0.715548
-29.467101	-1.410590	1.296243	0.005467	0.715540
-29.769174	-1.424099	1.301248	0.005523	0.715408
-30.349379	-1.413070	1.306253	0.005630	0.715225
-30.156235	-1.447259	1.311258	0.005594	0.715227
-30.389762	-1.403156	1.316262	0.005637	0.715232
-30.444664	-1.399530	1.321267	0.005647	0.715221
-30.144054	-1.447945	1.326272	0.005590	0.715232
-30.498733	-1.387492	1.331277	0.005656	0.715227
-30.871552	-1.427976	1.336282	0.005725	0.715016
-31.352180	-1.397510	1.341286	0.005814	0.714908
-31.405861	-1.392132	1.346291	0.005824	0.714900
-31.399336	-1.388002	1.351296	0.005822	0.714911
-31.753743	-1.328696	1.356301	0.005888	0.714905
-31.499051	-1.374598	1.361306	0.005840	0.714904
-31.283617	-1.411068	1.366310	0.005799	0.714909
-31.561598	-1.390466	1.371315	0.005851	0.714852
-31.956214	-1.443085	1.376320	0.005924	0.714609
-32.323258	-1.381249	1.381325	0.005991	0.714603
-32.840525	-1.288877	1.386330	0.006087	0.714604
-31.906190	-1.453189	1.391334	0.005913	0.714609
-32.162244	-1.412935	1.396339	0.005960	0.714599
-32.437206	-1.360704	1.401344	0.006011	0.714607
-32.293118	-1.389103	1.406349	0.005984	0.714602
-32.431065	-1.531647	1.411354	0.006009	0.714271
-33.133354	-1.404699	1.416358	0.006139	0.714275
-33.747401	-1.300033	1.421363	0.006253	0.714267
-32.913805	-1.443966	1.426368	0.006098	0.714277
-33.202863	-1.397082	1.431373	0.006151	0.714268
-33.763816	-1.296807	1.436378	0.006255	0.714270
-33.366231	-1.366283	1.441382	0.006181	0.714273
-33.467890	-1.445183	1.446387	0.006199	0.714081
-34.351990	-1.346208	1.451392	0.006363	0.713966
-34.397539	-1.341723	1.456397	0.006371	0.713960
-34.049356	-1.402086	1.461402	0.006306	0.713964
-33.980192	-1.412776	1.466406	0.006293	0.713968
-34.191474	-1.377861	1.471411	0.006332	0.713963
-34.004729	-1.408204	1.476416	0.006296	0.713970
-34.342850	-1.401309	1.481421	0.006359	0.713865
-35.475538	-1.309096	1.486426	0.006569	0.713647
-34.852004	-1.419108	1.491430	0.006453	0.713650
-34.880435	-1.417789	1.496435	0.006458	0.713644
-35.203768	-1.355450	1.501440	0.006518	0.713654
-35.135655	-1.370940	1.506445	0.006504	0.713648
-34.985918	-1.400462	1.511450	0.006476	0.713643
-34.681850	-1.474910	1.516454	0.006419	0.713604
-36.189386	-1.334110	1.521459	0.006699	0.713351
-35.654120	-1.426633	1.526464	0.006599	0.713357
-35.604204	-1.439625	1.531469	0.006590	0.713350
-35.757050	-1.411429	1.536474	0.006618	0.713352
-35.671929	-1.424730	1.541478	0.006601	0.713357
-35.834010	-1.400304	1.546483	0.006631	0.713349
-35.625255	-1.497779	1.551488	0.006592	0.713230
-36.888172	-1.381115	1.556493	0.006826	0.713015
-36.705451	-1.412513	1.561498	0.006792	0.713018
-36.473025	-1.451630	1.566502	0.006748	0.713023
-36.976228	-1.367049	1.571507	0.006842	0.713014
-36.551431	-1.438991	1.576512	0.006762	0.713022
-36.481783	-1.453066	1.581517	0.006749	0.713020
-37.014535	-1.440704	1.586522	0.006847	0.712856
-37.959607	-1.348388	1.591526	0.007023	0.712706
-37.554808	-1.424218	1.596531	0.006947	0.712699
-37.432619	-1.441264	1.601536	0.006924	0.712709
-37.859719	-1.368122	1.606541	0.007003	0.712704
-37.837087	-1.374016	1.611546	0.006998	0.712702
-37.427048	-1.444390	1.616550	0.006922	0.712708
-37.847378	-1.390329	1.621555	0.006999	0.712667
-38.298195	-1.451573	1.626560	0.007083	0.712386
-38.255126	-1.462909	1.631565	0.007075	0.712379
-38.765462	-1.372661	1.636570	0.007169	0.712379
-38.582642	-1.404393	1.641574	0.007135	0.712381
-38.559506	-1.414803	1.646579	0.007130	0.712370
-38.404850	-1.436854	1.651584	0.007101	0.712381
-38.623426	-1.410150	1.656589	0.007141	0.712358
-39.260836	-1.436240	1.661594	0.007259	0.712080
-39.104487	-1.461924	1.666598	0.007230	0.712086
-39.578536	-1.381077	1.671603	0.007318	0.712079
-39.359280	-1.416444	1.676608	0.007276	0.712087
-39.429291	-1.408609	1.681613	0.007289	0.712079
-39.462912	-1.401814	1.686618	0.007295	0.712081
-39.395753	-1.415249	1.691622	0.007282	0.712079
-39.929795	-1.487845	1.696627	0.007381	0.711746
-40.258070	-1.423653	1.701632	0.007442	0.711758
-40.834928	-1.324835	1.706637	0.007548	0.711751
-40.306652	-1.419653	1.711642	0.007450	0.711750
-39.899227	-1.488631	1.716646	0.007373	0.711758
-40.523197	-1.384902	1.721651	0.007489	0.711744
-40.273148	-1.424975	1.726656	0.007442	0.711754
-40.401517	-1.538632	1.731661	0.007466	0.711482
-41.191347	-1.417472	1.736666	0.007612	0.711444
-41.047734	-1.439365	1.741670	0.007585	0.711452
-41.471681	-1.368847	1.746675	0.007664	0.711443
-41.299858	-1.396746	1.751680	0.007631	0.711449
-41.382221	-1.385140	1.756685	0.007646	0.711444
-41.416350	-1.379195	1.761690	0.007652	0.711445
-41.410711	-1.488037	1.766694	0.007651	0.711230
-42.488937	-1.346881	1.771699	0.007851	0.711129
-42.175767	-1.401025	1.776704	0.007792	0.711134
-42.003796	-1.432863	1.781709	0.007760	0.711132
-42.351762	-1.371305	1.786714	0.007824	0.711132
-42.208250	-1.395334	1.791718	0.007797	0.711136
-42.233920	-1.396841	1.796723	0.007801	0.711125
-42.076163	-1.475185	1.801728	0.007771	0.711025
-43.169077	-1.362747	1.806733	0.007974	0.710862
-42.809272	-1.428605	1.811738	0.007907	0.710859
-42.555591	-1.469062	1.816742	0.007859	0.710869
-42.818820	-1.426903	1.821747	0.007908	0.710861
-42.814727	-1.424369	1.826752	0.007907	0.710868
-42.775159	-1.434410	1.831757	0.007899	0.710863
-43.063308	-1.518084	1.836762	0.007952	0.710594
-43.713549	-1.432942	1.841766	0.008073	0.710533
-44.025946	-1.382253	1.846771	0.008131	0.710524
-43.534215	-1.468925	1.851776	0.008039	0.710527
-43.875088	-1.408590	1.856781	0.008102	0.710527
-44.186627	-1.354146	1.861786	0.008159	0.710526
-43.712774	-1.435093	1.866790	0.008071	0.710533
-44.220391	-1.471465	1.871795	0.008165	0.710281
-45.035160	-1.357610	1.876800	0.008316	0.710219
-44.623585	-1.433515	1.881805	0.008239	0.710215
-44.614710	-1.439491	1.886810	0.008237	0.710207
-44.932240	-1.378159	1.891814	0.008296	0.710217
-44.808961	-1.405538	1.896819	0.008272	0.710207
-44.309235	-1.491685	1.901824	0.008179	0.710214
-44.890333	-1.506351	1.906829	0.008287	0.709978
-46.169359	-1.324849	1.911834	0.008524	0.709886
-45.432007	-1.453504	1.916838	0.008386	0.709893
-45.665498	-1.417612	1.921843	0.008430	0.709882
-46.066464	-1.343013	1.926848	0.008504	0.709889
-45.683164	-1.413138	1.931853	0.008432	0.709886
-45.500330	-1.447967	1.936858	0.008397	0.709883
-45.827617	-1.439429	1.941862	0.008458	0.709784
-46.899931	-1.348211	1.946867	0.008657	0.709585
-46.317647	-1.449625	1.951872	0.008548	0.709590
-46.492943	-1.420004	1.956877	0.008581	0.709588
-46.609466	-1.401833	1.961882	0.008602	0.709584
-46.172419	-1.475060	1.966886	0.008520	0.709594
-46.495919	-1.423202	1.971891	0.008580	0.709583
-46.616865	-1.456798	1.976896	0.008602	0.709474
-47.358326	-1.432960	1.981901	0.008740	0.709258
-47.335049	-1.438845	1.986906	0.008735	0.709255
-47.383423	-1.427397	1.991910	0.008743	0.709261
-47.752554	-1.365140	1.996915	0.008812	0.709255
-47.350397	-1.435930	2.001920	0.008736	0.709258

-47.325823	-1.461669	2.011917	0.008731	0.709217
-48.121051	-1.454516	2.021914	0.008878	0.708949
-48.462001	-1.395350	2.031910	0.008941	0.708947
-48.196956	-1.442627	2.041907	0.008891	0.708949
-48.020894	-1.473889	2.051904	0.008857	0.708951
-48.443411	-1.399913	2.061901	0.008935	0.708950
-48.282779	-1.429323	2.071898	0.008904	0.708950
-47.964499	-1.391497	2.081894	0.008844	0.709141
-47.585888	-1.401886	2.091891	0.008772	0.709257
-47.424494	-1.430963	2.101888	0.008742	0.709258
-47.576826	-1.403696	2.111885	0.008769	0.709260
-47.515208	-1.415693	2.121882	0.008757	0.709259
-47.756836	-1.375793	2.131878	0.008801	0.709255
-47.402442	-1.439071	2.141875	0.008734	0.709256
-47.289425	-1.401646	2.151872	0.008712	0.709373
-46.729834	-1.393169	2.161869	0.008607	0.709591
-46.648730	-1.409693	2.171866	0.008591	0.709588
-46.904744	-1.364614	2.181862	0.008638	0.709589
-46.707224	-1.399619	2.191859	0.008600	0.709591
-45.663771	-1.456349	2.201856	0.008405	0.709851
-45.719382	-1.426737	2.211853	0.008415	0.709892
-45.520040	-1.464881	2.221850	0.008377	0.709888
-46.186504	-1.345989	2.231846	0.008500	0.709890
-45.332672	-1.405385	2.241843	0.008340	0.710077
-45.079574	-1.381161	2.251840	0.008292	0.710218
-45.058568	-1.387015	2.261837	0.008287	0.710215
-44.857362	-1.424043	2.271834	0.008249	0.710214
-44.136064	-1.405433	2.281830	0.008114	0.710510
-43.912058	-1.436861	2.291827	0.008071	0.710529
-44.061370	-1.410838	2.301824	0.008098	0.710529
-44.106890	-1.378701	2.311821	0.008106	0.710579
-43.244715	-1.391768	2.321818	0.007944	0.710861
-43.215616	-1.396952	2.331814	0.007938	0.710863
-42.943789	-1.445468	2.341811	0.007887	0.710864
-43.094539	-1.343712	2.351808	0.007914	0.711015
-42.319810	-1.422680	2.361805	0.007769	0.711135
-42.535807	-1.385988	2.371802	0.007808	0.711133
-42.416640	-1.376519	2.381798	0.007785	0.711196
-41.458406	-1.421495	2.391795	0.007606	0.711448
-41.330922	-1.444209	2.401792	0.007581	0.711450
-41.365074	-1.440118	2.411789	0.007587	0.711448
-41.063639	-1.399398	2.421786	0.007530	0.711638
-40.747226	-1.399812	2.431782	0.007470	0.711751
-40.583177	-1.429432	2.441779	0.007439	0.711752
-40.686582	-1.379254	2.451776	0.007457	0.711817
-39.951494	-1.377835	2.461773	0.007319	0.712082
-39.717961	-1.420503	2.471770	0.007275	0.712082
-39.865602	-1.394897	2.481766	0.007302	0.712082
-39.202420	-1.388496	2.491763	0.007177	0.712332
-39.058794	-1.389683	2.501760	0.007150	0.712382
-39.006793	-1.400004	2.511757	0.007139	0.712382
-38.826164	-1.350339	2.521754	0.007105	0.712546
-38.211579	-1.382764	2.531750	0.006989	0.712701
-38.198462	-1.384586	2.541747	0.006986	0.712704
-38.280286	-1.335775	2.551744	0.007000	0.712774
-37.182969	-1.409500	2.561741	0.006795	0.713018
-37.261320	-1.397930	2.571738	0.006809	0.713015
-37.119798	-1.425104	2.581734	0.006782	0.713013
-36.603816	-1.410916	2.591731	0.006685	0.713225
-36.303292	-1.401366	2.601728	0.006628	0.713353
-36.191999	-1.421700	2.611725	0.006606	0.713353
-36.314815	-1.400245	2.621722	0.006628	0.713354
-35.621709	-1.378178	2.631718	0.006498	0.713645
-35.232520	-1.446963	2.641715	0.006425	0.713648
-35.560542	-1.390912	2.651712	0.006485	0.713645
-35.077145	-1.392517	2.661709	0.006395	0.713814
-34.793342	-1.369510	2.671706	0.006341	0.713962
-34.609470	-1.403050	2.681702	0.006306	0.713962
-34.524501	-1.401941	2.691699	0.006289	0.713996
-33.678798	-1.414077	2.701696	0.006131	0.714273
-33.722038	-1.407626	2.711693	0.006138	0.714272
-33.791309	-1.398386	2.721690	0.006150	0.714268
-33.265364	-1.397848	2.731686	0.006051	0.714457
-32.683096	-1.428611	2.741683	0.005942	0.714603
-32.714516	-1.424227	2.751680	0.005947	0.714602
-32.479797	-1.464934	2.761677	0.005902	0.714606
-32.388250	-1.358294	2.771674	0.005884	0.714852
-31.929983	-1.416618	2.781670	0.005798	0.714900
-32.032168	-1.399470	2.791667	0.005816	0.714899
-31.679172	-1.383626	2.801664	0.005750	0.715057
-31.059986	-1.409156	2.811661	0.005634	0.715227
-31.246605	-1.377361	2.821658	0.005668	0.715226
-31.021021	-1.404894	2.831654	0.005625	0.715252
-30.560883	-1.340270	2.841651	0.005538	0.715545
-29.953925	-1.449649	2.851648	0.005424	0.715544
-30.322362	-1.384991	2.861645	0.005492	0.715544
-29.586734	-1.405377	2.871642	0.005354	0.715765
-29.216964	-1.416156	2.881638	0.005285	0.715875
-29.187252	-1.422662	2.891635	0.005278	0.715875
-29.246147	-1.411216	2.901632	0.005288	0.715878
-28.633537	-1.396494	2.911629	0.005173	0.716125
-28.679302	-1.389003	2.921626	0.005181	0.716125
-28.472599	-1.425421	2.931622	0.005142	0.716128
-28.271215	-1.355313	2.941619	0.005103	0.716339
-27.699198	-1.404950	2.951616	0.004996	0.716445
-27.723574	-1.401230	2.961613	0.005000	0.716445
-27.482872	-1.390538	2.971610	0.004954	0.716553
-26.760269	-1.421064	2.981606	0.004819	0.716749
-26.764054	-1.421446	2.991603	0.004818	0.716748
-26.733875	-1.427404	3.001600	0.004812	0.716749
-26.161032	-1.380943	3.011597	0.004704	0.717044
-25.967148	-1.397021	3.021594	0.004667	0.717082
-25.832580	-1.424141	3.031590	0.004642	0.717078
-25.757457	-1.372762	3.041587	0.004627	0.717207
-24.724607	-1.473506	3.051584	0.004434	0.717374
-25.354234	-1.362926	3.061581	0.004550	0.717372
-25.062503	-1.415946	3.071578	0.004495	0.717372
-24.235095	-1.401244	3.081574	0.004340	0.717694
-24.281402	-1.393618	3.091571	0.004348	0.717694
-24.157453	-1.414261	3.101568	0.004324	0.717699
-23.806892	-1.384316	3.111565	0.004257	0.717883
-23.408963	-1.391343	3.121562	0.004183	0.718011
-23.281823	-1.415995	3.131558	0.004158	0.718008
-23.527031	-1.346280	3.141555	0.004203	0.718061
-22.592023	-1.368896	3.151552	0.004028	0.718347
-22.675465	-1.354063	3.161549	0.004042	0.718349
-22.472419	-1.391679	3.171546	0.004004	0.718347
-21.866906	-1.374352	3.181542	0.003890	0.718596
-21.739983	-1.376675	3.191539	0.003866	0.718638
-21.475726	-1.422897	3.201536	0.003816	0.718641
-21.486622	-1.363530	3.211533	0.003817	0.718756
-20.460353	-1.445700	3.221530	0.003625	0.718956
-20.677385	-1.407628	3.231526	0.003664	0.718957
-20.922210	-1.365716	3.241523	0.003709	0.718955
-20.020039	-1.400988	3.251520	0.003540	0.719204
-20.113656	-1.353551	3.261517	0.003557	0.719266
-19.805367	-1.411336	3.271514	0.003499	0.719262
-20.000912	-1.313720	3.281510	0.003534	0.719388
-18.842222	-1.415091	3.291507	0.003318	0.719596
-18.986019	-1.390301	3.301504	0.003344	0.719596
-18.917838	-1.403263	3.311501	0.003330	0.719596
-18.185127	-1.402161	3.321498	0.003193	0.719857
-18.201613	-1.382910	3.331494	0.003195	0.719891
-17.945774	-1.426396	3.341491	0.003146	0.719897
-17.921000	-1.382795	3.351488	0.003141	0.719993
-17.021476	-1.429496	3.361485	0.002973	0.720218
-17.205284	-1.398733	3.371482	0.003006	0.720216
-17.395385	-1.365103	3.381478	0.003040	0.720217
-16.469964	-1.406253	3.391475	0.002867	0.720462
-16.299017	-1.400911	3.401472	0.002835	0.720534
-16.213507	-1.417276	3.411469	0.002818	0.720533
-16.397393	-1.358549	3.421466	0.002851	0.720586
-15.672420	-1.344430	3.431462	0.002715	0.720870
-15.224912	-1.422755	3.441459	0.002631	0.720874
-15.616763	-1.356218	3.451456	0.002703	0.720869
-14.906986	-1.385186	3.461453	0.002570	0.721062
-14.673162	-1.397604	3.471450	0.002526	0.721121
-14.808006	-1.376795	3.481446	0.002550	0.721117
-14.450624	-1.372425	3.491443	0.002483	0.721252
-13.965382	-1.366400	3.501440	0.002392	0.721435
-13.756484	-1.404060	3.511437	0.002352	0.721436
-13.930968	-1.355561	3.521434	0.002383	0.721472
-13.143144	-1.359281	3.531430	0.002236	0.721742
-13.082017	-1.370667	3.541427	0.002224	0.721743
-13.144788	-1.359473	3.551424	0.002234	0.721744
-12.361610	-1.357414	3.561421	0.002088	0.722024
-12.102695	-1.380383	3.571418	0.002039	0.722071
-12.043095	-1.392292	3.581414	0.002027	0.722070
-11.878933	-1.371923	3.591411	0.001995	0.722169
-11.239608	-1.384008	3.601408	0.001875	0.722370
-11.119375	-1.407231	3.611405	0.001852	0.722368
-11.308253	-1.374340	3.621402	0.001887	0.722369
-10.515404	-1.377013	3.631398	0.001738	0.722642
-10.160239	-1.416020	3.641395	0.001671	0.722691
-10.378664	-1.377669	3.651392	0.001711	0.722692
-10.166628	-1.375537	3.661389	0.001671	0.722772
-9.493086	-1.378638	3.671386	0.001544	0.723002
-9.265051	-1.420019	3.681382	0.001501	0.723003
-9.196456	-1.434127	3.691379	0.001487	0.723000
-9.038969	-1.366468	3.701376	0.001457	0.723190
-8.191378	-1.440231	3.711373	0.001298	0.723343
-8.772853	-1.339315	3.721370	0.001406	0.723339
-8.327002	-1.416486	3.731366	0.001322	0.723345
-7.615425	-1.397622	3.741363	0.001189	0.723632
-7.593217	-1.401717	3.751360	0.001184	0.723633
-7.454253	-1.425602	3.761357	0.001157	0.723636
-7.403982	-1.363059	3.771354	0.001147	0.723778
-6.253895	-1.474245	3.781350	0.000932	0.723963
-6.427939	-1.445115	3.791347	0.000963	0.723961
-6.225734	-1.478941	3.801344	0.000925	0.723967
-6.158167	-1.425108	3.811341	0.000911	0.724097
-5.485389	-1.448634	3.821338	0.000785	0.724288
-5.172957	-1.503679	3.831334	0.000726	0.724290
-5.301478	-1.482615	3.841331	0.000749	0.724288
-5.196439	-1.452870	3.851328	0.000729	0.724385
-4.908035	-1.375892	3.861325	0.000674	0.724638
-4.748105	-1.405423	3.871322	0.000644	0.724637
-4.326623	-1.478002	3.881318	0.000564	0.724643
-4.140610	-1.388979	3.891315	0.000529	0.724884
-3.022624	-1.543596	3.901312	0.000320	0.724972
-3.370267	-1.484045	3.911309	0.000384	0.724969
-3.227772	-1.509192	3.921306	0.000356	0.724972
-3.957343	-1.291730	3.931302	0.000491	0.725144
-3.389923	-1.320612	3.941299	0.000385	0.725287
-2.966710	-1.392214	3.951296	0.000305	0.725296
-2.490901	-1.356263	3.961293	0.000216	0.725533
-1.692528	-1.461251	3.971290	0.000066	0.725608
-1.736959	-1.456001	3.981286	0.000074	0.725604
-2.165797	-1.371320	3.991283	0.000152	0.725622
-2.714040	-1.109804	4.001280	0.000254	0.725944
-1.863382	-1.263770	4.011277	0.000094	0.725940
-2.110698	-1.135324	4.021274	0.000140	0.726107
-1.593090	-1.175568	4.031270	0.000042	0.726210
-1.149153	-1.231752	4.041267	-0.000041	0.726256
-0.918624	-1.138873	4.051264	-0.000085	0.726519
-0.862099	-1.149193	4.061261	-0.000096	0.726520
-1.297931	-0.967334	4.071258	-0.000016	0.726725
-0.760257	-1.014144	4.081254	-0.000117	0.726822
-0.676434	-0.932314	4.091251	-0.000134	0.727012
-0.694342	-0.858125	4.101248	-0.000131	0.727152
-0.688389	-0.766440	4.111245	-0.000133	0.727335
-0.437471	-0.753541	4.121242	-0.000181	0.727448
-0.361714	-0.641551	4.131238	-0.000196	0.727695
-0.545430	-0.556477	4.141235	-0.000163	0.727798
-0.256389	-0.463285	4.151232	-0.000217	0.728081
-0.295497	-0.369882	4.161229	-0.000211	0.728251
-0.180303	-0.306250	4.171226	-0.000233	0.728417
0.029367	-0.193662	4.181222	-0.000273	0.728710
-0.118018	-0.072997	4.191219	-0.000247	0.728895
0.143311	-0.018980	4.201216	-0.000296	0.729092
0.000000	0.177814	4.211213	-0.000271	0.729427

0.229942	0.762452	4.216218	-0.000314	0.730643
0.347862	2.017400	4.221222	-0.000337	0.733115
0.971121	3.787249	4.226227	-0.000455	0.736744
1.551061	6.117386	4.231232	-0.000565	0.741412
1.868569	9.021013	4.236237	-0.000626	0.747051
2.424968	12.378369	4.241242	-0.000733	0.753582
2.881808	16.177749	4.246246	-0.000821	0.760848
3.556010	20.375126	4.251251	-0.000949	0.768850
4.110711	24.981845	4.256256	-0.001056	0.777478
5.227058	29.864886	4.261261	-0.001268	0.786688
6.377717	35.100729	4.266266	-0.001486	0.796430
6.679431	40.799300	4.271270	-0.001546	0.806604
7.406713	46.741213	4.276275	-0.001686	0.817203
7.859904	53.001550	4.281280	-0.001775	0.828128
8.749611	59.464346	4.286285	-0.001945	0.839383
9.268708	66.205272	4.291290	-0.002046	0.850843
10.372443	73.061793	4.296294	-0.002257	0.862510
11.218989	80.187631	4.301299	-0.002419	0.874383
11.686195	87.541099	4.306304	-0.002512	0.886355
12.412173	95.033679	4.311309	-0.002652	0.898457
12.940120	102.733336	4.316314	-0.002756	0.910667
13.415697	110.546094	4.321318	-0.002850	0.922874
14.323418	118.419082	4.326323	-0.003025	0.935128
14.895365	126.457309	4.331328	-0.003137	0.947382
15.383050	134.624375	4.336333	-0.003233	0.959648
16.072046	142.834694	4.341338	-0.003367	0.971873
16.706849	151.121886	4.346342	-0.003491	0.984043
17.342832	159.524298	4.351347	-0.003616	0.996227
18.000411	167.909042	4.356352	-0.003744	1.008245
19.014293	176.307986	4.361357	-0.003939	1.020226
19.529898	184.845913	4.366362	-0.004041	1.032140
19.865209	193.423060	4.371366	-0.004109	1.043929
20.455829	202.006983	4.376371	-0.004225	1.055654
21.325600	210.552115	4.381376	-0.004393	1.067262
22.101354	219.151729	4.386381	-0.004544	1.078795
22.820566	227.762639	4.391386	-0.004684	1.090208
23.261429	236.412262	4.396390	-0.004772	1.101490
24.029345	245.032729	4.401395	-0.004921	1.112693
25.077002	253.584849	4.406400	-0.005122	1.123757
25.557685	262.261767	4.411405	-0.005217	1.134747
26.076398	270.915648	4.416410	-0.005320	1.145612
26.549531	279.607358	4.421414	-0.005414	1.156410
27.119133	288.217474	4.426419	-0.005526	1.167030
27.715603	296.822541	4.431424	-0.005643	1.177553
28.319674	305.420043	4.436429	-0.005762	1.187975
28.606540	314.070590	4.441434	-0.005821	1.198304
29.163933	322.631195	4.446438	-0.005931	1.208494
30.071318	331.155868	4.451443	-0.006106	1.218626
30.611363	339.717016	4.456448	-0.006213	1.228644
30.931284	348.313458	4.461453	-0.006278	1.238578
31.570508	356.822495	4.466458	-0.006403	1.248395
31.961029	365.367849	4.471462	-0.006482	1.258129
32.771598	373.839145	4.476467	-0.006639	1.267785
33.487964	382.313378	4.481472	-0.006778	1.277352
34.263668	390.755405	4.486477	-0.006929	1.286824
34.701574	399.271853	4.491482	-0.007016	1.296245
35.171370	407.743861	4.496486	-0.007110	1.305556
36.052156	416.274328	4.501491	-0.007280	1.314938
36.633607	424.688577	4.506496	-0.007394	1.324075
36.975020	433.139238	4.511501	-0.007463	1.333146
37.288183	441.578232	4.516506	-0.007528	1.342137
37.464801	450.017953	4.521510	-0.007566	1.351045
38.472660	458.323606	4.526515	-0.007760	1.359900
39.019946	466.692665	4.531520	-0.007868	1.368683
39.375478	475.099140	4.536525	-0.007940	1.377416
39.919217	483.456234	4.541530	-0.008047	1.386074
40.493175	491.830282	4.546534	-0.008160	1.394702
41.262658	500.135321	4.551539	-0.008309	1.403239
41.489018	508.517636	4.556544	-0.008357	1.411711
42.129208	516.828470	4.561549	-0.008482	1.420130
42.720677	525.151845	4.566554	-0.008598	1.428503
42.695169	533.559432	4.571558	-0.008599	1.436810
43.516889	541.802588	4.576563	-0.008758	1.445044
43.816240	550.140833	4.581568	-0.008819	1.453241
44.420723	558.423352	4.586573	-0.008938	1.461386
44.874345	566.755708	4.591578	-0.009028	1.469510
45.182604	575.103152	4.596582	-0.009091	1.477581
45.781988	583.339835	4.601587	-0.009209	1.485547
46.286061	591.625488	4.606592	-0.009308	1.493503
46.641302	599.903229	4.611597	-0.009380	1.501386
47.136958	608.177979	4.616602	-0.009479	1.509246
47.618951	616.437921	4.621606	-0.009574	1.517049
48.084401	624.687786	4.626611	-0.009667	1.524800
48.573980	632.941727	4.631616	-0.009764	1.532520
49.081027	641.182317	4.636621	-0.009864	1.540190
49.594097	649.417800	4.641626	-0.009965	1.547819
49.822228	657.711417	4.646630	-0.010013	1.555421
50.298588	665.930164	4.651635	-0.010108	1.562955
50.610074	674.166135	4.656640	-0.010172	1.570444
50.996510	682.408712	4.661645	-0.010249	1.577913
51.368265	690.628035	4.666650	-0.010324	1.585325
51.850984	698.848620	4.671654	-0.010420	1.592719
52.517796	707.032746	4.676659	-0.010550	1.600073
52.792032	715.262000	4.681664	-0.010607	1.607377
53.227805	723.484290	4.686669	-0.010694	1.614664
53.714314	731.690729	4.691674	-0.010790	1.621912
53.644999	739.979534	4.696678	-0.010783	1.629121
54.171473	748.212410	4.701683	-0.010887	1.636333
54.414273	756.403543	4.706688	-0.010938	1.643438
54.989460	764.551282	4.711693	-0.011051	1.650521
55.223741	772.775598	4.716698	-0.011100	1.657592
55.282859	780.975805	4.721702	-0.011117	1.664589
55.701469	789.170713	4.726707	-0.011201	1.671600
56.022347	797.341240	4.731712	-0.011266	1.678549
56.490447	805.477911	4.736717	-0.011359	1.685459
56.970987	813.668385	4.741722	-0.011454	1.692388
57.128237	821.866832	4.746726	-0.011489	1.699253
57.710315	830.010376	4.751731	-0.011603	1.706100
58.493410	838.152972	4.756736	-0.011755	1.712945
59.174972	846.275174	4.761741	-0.011888	1.719732
59.766531	854.432542	4.766746	-0.012003	1.726510
60.069098	862.636424	4.771750	-0.012066	1.733262
60.448981	870.814283	4.776755	-0.012142	1.739976
60.504522	879.026191	4.781760	-0.012158	1.746651
60.996860	887.191462	4.786765	-0.012256	1.753318
61.555532	895.323056	4.791770	-0.012365	1.759941
61.783863	903.484586	4.796774	-0.012414	1.766521
62.167011	911.671083	4.801779	-0.012491	1.773116
62.602560	919.803972	4.806784	-0.012578	1.779650
62.705881	927.989273	4.811789	-0.012603	1.786161
63.095909	936.195488	4.816794	-0.012681	1.792700
63.186885	944.380391	4.821798	-0.012704	1.799162
63.574264	952.469715	4.826803	-0.012782	1.805562
63.772534	960.640152	4.831808	-0.012824	1.811979
64.266354	968.752642	4.836813	-0.012922	1.818364
64.810731	976.859183	4.841818	-0.013029	1.824728
65.081647	985.007587	4.846822	-0.013085	1.831070
65.368323	993.174403	4.851827	-0.013144	1.837405
65.683963	1001.295912	4.856832	-0.013209	1.843688
65.839393	1009.458591	4.861837	-0.013243	1.849961
66.123451	1017.617373	4.866842	-0.013302	1.856226
66.288265	1025.744802	4.871846	-0.013338	1.862432
66.697037	1033.874616	4.876851	-0.013420	1.868647
67.177605	1042.004605	4.881856	-0.013516	1.874849
67.567690	1050.100867	4.886861	-0.013594	1.880995
68.048902	1058.209706	4.891866	-0.013689	1.887141
67.984162	1066.400221	4.896870	-0.013683	1.893266
68.260314	1074.531129	4.901875	-0.013740	1.899366
68.623450	1082.621032	4.906880	-0.013813	1.905425
69.125865	1090.738508	4.911885	-0.013913	1.911500
69.370871	1098.875933	4.916890	-0.013964	1.917543
69.486510	1107.001723	4.921894	-0.013991	1.923543
69.887373	1115.119365	4.926899	-0.014072	1.929550
70.155363	1123.254294	4.931904	-0.014127	1.935537
70.336773	1131.372860	4.936909	-0.014167	1.941483
70.843183	1139.467894	4.941914	-0.014267	1.947430
71.116360	1147.631092	4.946918	-0.014323	1.953382
71.500301	1155.738877	4.951923	-0.014401	1.959288
71.745979	1163.809566	4.956928	-0.014452	1.965135
72.467166	1171.871956	4.961933	-0.014592	1.971009
72.863112	1180.005820	4.966938	-0.014671	1.976883
73.091750	1188.107794	4.971942	-0.014720	1.982698
73.329357	1196.238795	4.976947	-0.014770	1.988517
73.761095	1204.348921	4.981952	-0.014856	1.994325
74.313338	1212.403178	4.986957	-0.014964	2.000090
74.687894	1220.514349	4.991962	-0.015040	2.005859
75.036495	1228.623751	4.996966	-0.015110	2.011607
75.354183	1236.747428	5.001971	-0.015175	2.017346
75.647698	1244.844744	5.006976	-0.015236	2.023048
76.050595	1252.950155	5.011981	-0.015316	2.028750
76.290888	1261.120396	5.016986	-0.015367	2.034465
76.508246	1269.201951	5.021990	-0.015413	2.040100
76.790640	1277.293559	5.026995	-0.015471	2.045732
76.904567	1285.422013	5.032000	-0.015498	2.051358
77.248086	1293.504993	5.037005	-0.015568	2.056960
77.714374	1301.573684	5.042010	-0.015660	2.062549
77.934931	1309.673390	5.047014	-0.015707	2.068120
78.027448	1317.837147	5.052019	-0.015730	2.073706
78.388660	1325.898752	5.057024	-0.015803	2.079235
78.727089	1333.968637	5.062029	-0.015872	2.084752
78.857082	1342.099233	5.067034	-0.015902	2.090275
79.202724	1350.179927	5.072038	-0.015972	2.095771
79.664092	1358.252599	5.077043	-0.016063	2.101258
79.920275	1366.347615	5.082048	-0.016117	2.106726
80.086994	1374.501745	5.087053	-0.016154	2.112211
80.647556	1382.582061	5.092058	-0.016264	2.117670
80.712619	1390.655515	5.097062	-0.016281	2.123063
80.943469	1398.750367	5.102067	-0.016330	2.128472
81.301844	1406.838494	5.107072	-0.016403	2.133875
81.709511	1414.890998	5.112077	-0.016484	2.139246
81.719854	1423.007048	5.117082	-0.016492	2.144607
81.940497	1431.082252	5.122086	-0.016539	2.149948
82.503550	1439.161599	5.127091	-0.016649	2.155310
82.843010	1447.223323	5.132096	-0.016718	2.160627
82.978387	1455.319923	5.137101	-0.016749	2.165934
83.422838	1463.409516	5.142106	-0.016837	2.171252
83.655127	1471.488199	5.147110	-0.016886	2.176530
83.888105	1479.587066	5.152115	-0.016935	2.181809
84.238103	1487.659942	5.157120	-0.017006	2.187069
84.585569	1495.764014	5.162125	-0.017077	2.192336
85.041489	1503.847779	5.167130	-0.017167	2.197587
85.346840	1511.901497	5.172134	-0.017230	2.202792
85.509048	1519.985911	5.177139	-0.017266	2.207992
85.692969	1528.099894	5.182144	-0.017306	2.213201
85.834843	1536.181761	5.187149	-0.017338	2.218372
86.050792	1544.258221	5.192154	-0.017384	2.223536
86.269953	1552.330052	5.197158	-0.017430	2.228684
86.519519	1560.436927	5.202163	-0.017482	2.233845
86.765302	1568.490873	5.207168	-0.017534	2.238961
87.198471	1576.517702	5.212173	-0.017620	2.244064
87.378535	1584.631427	5.217178	-0.017659	2.249188
87.716308	1592.690340	5.222182	-0.017728	2.254280
87.909204	1600.796347	5.227187	-0.017770	2.259377
88.336630	1608.845265	5.232192	-0.017855	2.264447
88.533348	1616.923979	5.237197	-0.017897	2.269504
88.568012	1625.131166	5.242202	-0.017909	2.274616
88.942731	1633.124916	5.247206	-0.017985	2.279613
89.300366	1641.156742	5.252211	-0.018057	2.284622
89.413948	1649.237820	5.257216	-0.018084	2.289628
89.614395	1657.329030	5.262221	-0.018127	2.294638
90.041804	1665.369822	5.267226	-0.018212	2.299625
90.158549	1673.437947	5.272230	-0.018240	2.304591
90.669594	1681.492473	5.277235	-0.018340	2.309572
90.977099	1689.578302	5.282240	-0.018403	2.314544
91.096172	1697.641950	5.287245	-0.018431	2.319475
91.622032	1705.681711	5.292250	-0.018535	2.324416
91.832822	1713.744345	5.297254	-0.018580	2.329334
92.009242	1721.873686	5.302259	-0.018618	2.334279
92.234582	1729.922347	5.307264	-0.018666	2.339168
92.663160	1737.958626	5.312269	-0.018751	2.344057
93.058257	1746.039339	5.317274	-0.018831	2.348959
93.197118	1754.158889	5.322278	-0.018862	2.353854
93.403432	1762.220459	5.327283	-0.018906	2.358709
93.595711	1770.264938	5.332288	-0.018948	2.363543
93.916797	1778.331161	5.337293	-0.019013	2.368390
94.311302	1786.405307	5.342298	-0.019092	2.373237
94.719638	1794.450016	5.347302	-0.019174	2.378059
95.005733	1802.498268	5.352307	-0.019233	2.382862
95.113636	1810.588936	5.357312	-0.019259	2.387667
95.260121	1818.681848	5.362317	-0.019292	2.392467
95.927837	1826.710670	5.367322	-0.019422	2.397261
96.075788	1834.766714	5.372326	-0.019455	2.402019
96.271880	1842.855816	5.377331	-0.019497	2.406792
96.583307	1850.938329	5.382336	-0.019561	2.411560
96.616606	1859.015022	5.387341	-0.019573	2.416294
97.029900	1867.050537	5.392346	-0.019655	2.421024
97.353020	1875.093093	5.397350	-0.019721	2.425742
97.535239	1883.205033	5.402355	-0.019761	2.430479
97.697994	1891.335232	5.407360	-0.019797	2.435217
98.059877	1899.324768	5.412365	-0.019870	2.439880
98.225070	1907.375950	5.417370	-0.019906	2.444553
98.236737	1915.439304	5.422374	-0.019914	2.449214
98.525365	1923.505002	5.427379	-0.019974	2.453888
98.738345	1931.563339	5.432384	-0.020019	2.458543
98.876821	1939.594083	5.437389	-0.020050	2.463167
99.354045	1947.635287	5.442394	-0.020145	2.467814
99.773685	1955.676544	5.447398	-0.020229	2.472449
100.055592	1963.757390	5.452403	-0.020287	2.477086
100.308345	1971.807219	5.457408	-0.020340	2.481695
100.617705	1979.828875	5.462413	-0.020403	2.486284
100.977036	1987.915185	5.467418	-0.020476	2.490905
101.072519	1996.002677	5.472422	-0.020499	2.495498
101.412727	2004.050882	5.477427	-0.020568	2.500078
101.504084	2012.104698	5.482432	-0.020591	2.504635
101.553059	2020.178712	5.487437	-0.020606	2.509193
102.023755	2028.273702	5.492442	-0.020699	2.513784
102.176671	2036.325624	5.497446	-0.020733	2.518319
102.439078	2044.345533	5.502451	-0.020788	2.522836
102.761889	2052.386488	5.507456	-0.020853	2.527361
102.810489	2060.466782	5.512461	-0.020868	2.531881
103.324951	2068.508802	5.517466	-0.020970	2.536404
103.683092	2076.541946	5.522470	-0.021042	2.540903
103.711600	2084.603124	5.527475	-0.021053	2.545386
104.182634	2092.649901	5.532480	-0.021146	2.549885
104.368061	2100.720914	5.537485	-0.021187	2.554369
104.626360	2108.776657	5.542490	-0.021240	2.558841
105.007815	2116.773342	5.547494	-0.021317	2.563282
105.341922	2124.835485	5.552499	-0.021385	2.567748
105.270354	2132.955934	5.557504	-0.021377	2.572209
105.417133	2141.017432	5.562509	-0.021410	2.576646
106.122607	2149.018133	5.567514	-0.021547	2.581081
106.411454	2157.066194	5.572518	-0.021607	2.585504
106.797579	2165.139201	5.577523	-0.021684	2.589941
107.163081	2173.386170	5.582528	-0.021758	2.594463
107.210033	2181.379602	5.587533	-0.021773	2.598818
107.342951	2189.396743	5.592538	-0.021803	2.603184
107.641397	2197.392997	5.597542	-0.021864	2.607543
108.120633	2205.420722	5.602547	-0.021959	2.611923
108.362754	2213.484146	5.607552	-0.022010	2.616300
108.694788	2221.491040	5.612557	-0.022077	2.620644
109.174940	2229.519191	5.617562	-0.022172	2.625003
109.281027	2237.589777	5.622566	-0.022198	2.629352
109.590756	2245.667003	5.627571	-0.022261	2.633711
109.987457	2253.686493	5.632576	-0.022341	2.638038
110.051902	2261.730777	5.637581	-0.022358	2.642349
110.268924	2269.790559	5.642586	-0.022404	2.646671
110.223239	2277.862773	5.647590	-0.022402	2.650975
110.715056	2285.914859	5.652595	-0.022499	2.655297
110.901163	2293.952510	5.657600	-0.022539	2.659584
110.994536	2301.991613	5.662605	-0.022562	2.663859
111.467662	2310.032213	5.667610	-0.022656	2.668152
111.572848	2318.120761	5.672614	-0.022681	2.672440
111.656208	2326.191318	5.677619	-0.022703	2.676711
112.113084	2334.185131	5.682624	-0.022793	2.680958
112.201082	2342.206878	5.687629	-0.022815	2.685189
112.519632	2350.260416	5.692634	-0.022880	2.689445
112.763894	2358.337058	5.697638	-0.022931	2.693701
112.821653	2366.397833	5.702643	-0.022948	2.697931
112.940742	2374.443632	5.707648	-0.022976	2.702150
113.104679	2382.479363	5.712653	-0.023012	2.706360
113.596246	2390.520780	5.717658	-0.023109	2.710587
113.793543	2398.568872	5.722662	-0.023152	2.714792
113.970726	2406.622358	5.727667	-0.023190	2.718993
114.148219	2414.651075	5.732672	-0.023229	2.723174
114.395122	2422.695425	5.737677	-0.023281	2.727361
114.654109	2430.760506	5.742682	-0.023334	2.731552
114.698914	2438.824874	5.747686	-0.023349	2.735724
115.154969	2446.843781	5.752691	-0.023439	2.739892
115.548746	2454.856467	5.757696	-0.023518	2.744045
115.491234	2462.931785	5.762701	-0.023513	2.748198
115.895837	2471.025009	5.767706	-0.023594	2.752381
116.045534	2479.109634	5.772710	-0.023628	2.756538
116.386120	2487.109720	5.777715	-0.023697	2.760657
116.697207	2495.087544	5.782720	-0.023760	2.764756
117.026271	2503.097311	5.787725	-0.023827	2.768867
117.296886	2511.189724	5.792730	-0.023883	2.773010
117.365611	2519.257226	5.797734	-0.023902	2.777122
117.487284	2527.294925	5.802739	-0.023930	2.781217
117.856958	2535.300310	5.807744	-0.024005	2.785303
118.212830	2543.319271	5.812749	-0.024076	2.789389
118.587625	2551.407256	5.817754	-0.024152	2.793506
118.578860	2559.447329	5.822758	-0.024156	2.797569
118.687174	2567.502898	5.827763	-0.024182	2.801642
118.972966	2575.525609	5.832768	-0.024241	2.805702
119.213205	2583.557905	5.837773	-0.024291	2.809758
119.397706	2591.646284	5.842778	-0.024331	2.813834
119.313541	2599.720680	5.847782	-0.024321	2.817881
119.656676	2607.725888	5.852787	-0.024391	2.821912
120.064573	2615.761560	5.857792	-0.024472	2.825956
120.158748	2623.788525	5.862797	-0.024496	2.829972
120.592203	2631.872186	5.867802	-0.024582	2.834030
120.896734	2639.900207	5.872806	-0.024644	2.838047
121.153163	2647.921381	5.877811	-0.024698	2.842053
121.269345	2655.974327	5.882816	-0.024725	2.846060
121.397856	2663.985660	5.887821	-0.024755	2.850042
121.838230	2672.042401	5.892826	-0.024842	2.854058
121.892803	2680.085431	5.897830	-0.024858	2.858040
122.208847	2688.091297	5.902835	-0.024923	2.862013
122.323835	2696.137406	5.907840	-0.024950	2.865989
122.397415	2704.187993	5.912845	-0.024969	2.869959
122.900316	2712.258194	5.917850	-0.025068	2.873957
123.053793	2720.277249	5.922854	-0.025103	2.877905
123.270663	2728.309245	5.927859	-0.025149	2.881858
123.463484	2736.352525	5.932864	-0.025190	2.885809
123.752750	2744.366836	5.937869	-0.025250	2.889746
124.239889	2752.423340	5.942874	-0.025346	2.893708
124.151060	2760.508915	5.947878	-0.025335	2.897649
124.243119	2768.541837	5.952883	-0.025358	2.901568
124.491920	2776.567718	5.957888	-0.025410	2.905486
124.708969	2784.590077	5.962893	-0.025456	2.909396
125.133272	2792.743461	5.967898	-0.025541	2.913376
125.327007	2800.757572	5.972902	-0.025583	2.917270
125.690753	2808.742551	5.977907	-0.025656	2.921154
125.917035	2816.735313	5.982912	-0.025704	2.925029
126.159512	2824.753215	5.987917	-0.025755	2.928911
126.530358	2832.820386	5.992922	-0.025829	2.932820
126.611119	2840.858733	5.997926	-0.025850	2.936693
126.842267	2848.883595	6.002931	-0.025899	2.940563
127.291760	2856.879847	6.007936	-0.025988	2.944426
127.350455	2864.950035	6.012941	-0.026005	2.948298
127.615836	2873.018309	6.017946	-0.026060	2.952176
128.042200	2881.043378	6.022950	-0.026145	2.956035
128.264528	2889.057982	6.027955	-0.026192	2.959875
128.461710	2897.086477	6.032960	-0.026234	2.963714
128.452921	2905.144987	6.037965	-0.026238	2.967552
128.992062	2913.197900	6.042970	-0.026344	2.971411
129.024479	2921.238844	6.047974	-0.026356	2.975233
129.275397	2929.281308	6.052979	-0.026408	2.979061
129.787515	2937.278074	6.057984	-0.026509	2.982877
129.785184	2945.340085	6.062989	-0.026515	2.986692
130.055324	2953.396038	6.067994	-0.026571	2.990514
130.012356	2961.496294	6.072998	-0.026568	2.994335
130.199938	2969.505627	6.078003	-0.026609	2.998121
130.582117	2977.508620	6.083008	-0.026686	3.001908
130.854756	2985.494279	6.088013	-0.026742	3.005677
131.104054	2993.531812	6.093018	-0.026794	3.009464
131.165912	3001.615277	6.098022	-0.026811	3.013259
131.439121	3009.640140	6.103027	-0.026868	3.017032
131.767649	3017.683433	6.108032	-0.026935	3.020811
131.732388	3025.711461	6.113037	-0.026934	3.024561
131.820986	3033.786063	6.118042	-0.026956	3.028334
131.943084	3041.806987	6.123046	-0.026985	3.032079
132.270726	3049.848762	6.128051	-0.027051	3.035839
132.381646	3057.874776	6.133056	-0.027077	3.039576
132.682113	3065.877670	6.138061	-0.027139	3.043307
132.892906	3073.928096	6.143066	-0.027184	3.047051
132.937641	3081.971266	6.148070	-0.027198	3.050780
133.225614	3090.018188	6.153075	-0.027257	3.054517
133.483796	3098.051141	6.158080	-0.027311	3.058241
133.532414	3106.062714	6.163085	-0.027326	3.061942
134.020354	3114.066177	6.168090	-0.027422	3.065654
134.083198	3122.133858	6.173094	-0.027440	3.069372
134.319886	3130.226253	6.178099	-0.027489	3.073105
134.607881	3138.274430	6.183104	-0.027549	3.076815
134.828945	3146.253473	6.188109	-0.027595	3.080486
135.129384	3154.260701	6.193114	-0.027657	3.084169
135.289119	3162.276873	6.198118	-0.027692	3.087845
135.434946	3170.329377	6.203123	-0.027725	3.091533
135.753310	3178.376251	6.208128	-0.027790	3.095221
135.868917	3186.410123	6.213133	-0.027817	3.098890
136.032299	3194.432329	6.218138	-0.027854	3.102552
136.274582	3202.449334	6.223142	-0.027904	3.106210
136.567554	3210.486668	6.228147	-0.027965	3.109876
136.690548	3218.573312	6.233152	-0.027993	3.113551
136.629767	3226.590717	6.238157	-0.027987	3.117183
137.102231	3234.599647	6.243162	-0.028081	3.120831
137.344214	3242.605136	6.248166	-0.028132	3.124462
137.313396	3250.643612	6.253171	-0.028132	3.128092
137.834836	3258.697789	6.258176	-0.028234	3.131750
138.014471	3266.732276	6.263181	-0.028274	3.135379
138.056607	3274.773045	6.268186	-0.028287	3.139000
137.874386	3282.812508	6.273190	-0.028259	3.142607
138.178164	3290.838532	6.278195	-0.028321	3.146225
138.527997	3298.876416	6.283200	-0.028392	3.149847
138.534286	3306.953085	6.288205	-0.028399	3.153466
138.764458	3314.987223	6.293210	-0.028447	3.157072
139.116708	3322.959405	6.298214	-0.028518	3.160651
139.180598	3330.971587	6.303219	-0.028536	3.164232
139.630765	3338.973688	6.308224	-0.028625	3.167821
139.568536	3347.060557	6.313229	-0.028620	3.171421
139.694841	3355.106822	6.318234	-0.028649	3.175007
139.868234	3363.139452	6.323238	-0.028687	3.178585
140.254285	3371.121402	6.328243	-0.028764	3.182146
140.607509	3379.152265	6.333248	-0.028836	3.185723
140.726288	3387.185856	6.338253	-0.028863	3.189287
141.184706	3395.251843	6.343258	-0.028955	3.192876
141.289081	3403.298682	6.348262	-0.028980	3.196437
141.307204	3411.299080	6.353267	-0.028989	3.199970
141.564815	3419.338027	6.358272	-0.029042	3.203526
141.805959	3427.343639	6.363277	-0.029093	3.207063
141.906118	3435.412711	6.368282	-0.029117	3.210618
141.915716	3443.460949	6.373286	-0.029125	3.214156
142.278298	3451.467775	6.378291	-0.029198	3.217687
142.538474	3459.492487	6.383296	-0.029252	3.221217
142.753398	3467.481896	6.388301	-0.029298	3.224727
142.835171	3475.571804	6.393306	-0.029318	3.228270
143.133758	3483.628978	6.398310	-0.029380	3.231805
143.227601	3491.698458	6.403315	-0.029403	3.235332
143.421104	3499.700221	6.408320	-0.029445	3.238831
143.578942	3507.693254	6.413325	-0.029480	3.242320
143.867913	3515.724472	6.418330	-0.029539	3.245827
143.796801	3523.744615	6.423334	-0.029531	3.249311
144.041005	3531.781680	6.428339	-0.029583	3.252811
144.359547	3539.837255	6.433344	-0.029648	3.256319
144.331249	3547.814577	6.438349	-0.029648	3.259775
144.763430	3555.850551	6.443354	-0.029734	3.263271
145.003482	3563.868855	6.448358	-0.029784	3.266748
145.170344	3571.903224	6.453363	-0.029821	3.270225
145.228787	3579.982159	6.458368	-0.029838	3.273714
145.516546	3587.981534	6.463373	-0.029897	3.277173
145.760389	3595.983331	6.468378	-0.029948	3.280629
145.871949	3603.991126	6.473382	-0.029974	3.284077
146.213979	3612.009146	6.478387	-0.030044	3.287536
146.562010	3620.078907	6.483392	-0.030114	3.291013
146.574891	3628.121190	6.488397	-0.030122	3.294462
146.939788	3636.144010	6.493402	-0.030196	3.297913
147.071553	3644.168525	6.498406	-0.030226	3.301351
147.170111	3652.167171	6.503411	-0.030250	3.304774
147.528103	3660.216904	6.508416	-0.030322	3.308225
147.664997	3668.269236	6.513421	-0.030354	3.311664
148.102863	3676.312862	6.518426	-0.030441	3.315108
148.140966	3684.334386	6.523430	-0.030454	3.318524
148.396225	3692.315649	6.528435	-0.030507	3.321927
148.618784	3700.331640	6.533440	-0.030554	3.325341
148.659490	3708.380795	6.538445	-0.030567	3.328758
148.827161	3716.446275	6.543450	-0.030604	3.332183
149.037715	3724.464018	6.548454	-0.030649	3.335586
149.308438	3732.469298	6.553459	-0.030705	3.338982
149.441242	3740.530360	6.558464	-0.030735	3.342394
149.703500	3748.498947	6.563469	-0.030790	3.345767
149.925659	3756.573254	6.568474	-0.030837	3.349181
150.192746	3764.591969	6.573478	-0.030892	3.352569
150.167529	3772.669395	6.578483	-0.030893	3.355967
150.346856	3780.675726	6.583488	-0.030932	3.359340
150.477282	3788.682499	6.588493	-0.030962	3.362708
150.641085	3796.730240	6.593498	-0.030998	3.366090
150.889953	3804.740882	6.598502	-0.031050	3.369457
151.262174	3812.755848	6.603507	-0.031125	3.372827
151.445127	3820.833959	6.608512	-0.031165	3.376212
151.783545	3828.809898	6.613517	-0.031234	3.379558
152.014617	3836.852387	6.618522	-0.031282	3.382923
152.266933	3844.866007	6.623526	-0.031335	3.386275
152.431119	3852.890630	6.628531	-0.031371	3.389624
152.746707	3860.993080	6.633536	-0.031436	3.393007
152.644347	3869.048730	6.638541	-0.031422	3.396354
152.899403	3877.001885	6.643546	-0.031475	3.399666
152.944292	3885.023393	6.648550	-0.031489	3.402997
153.109889	3893.048750	6.653555	-0.031526	3.406330
153.534632	3901.039377	6.658560	-0.031611	3.409654
153.427700	3909.102522	6.663565	-0.031596	3.412987
153.874314	3917.142781	6.668570	-0.031685	3.416326
153.960148	3925.127897	6.673574	-0.031707	3.419627
153.990249	3933.160195	6.678579	-0.031718	3.422942
154.475786	3941.195442	6.683584	-0.031814	3.426270
154.701823	3949.187200	6.688589	-0.031862	3.429568
154.620682	3957.299225	6.693594	-0.031853	3.432903
154.715446	3965.326461	6.698598	-0.031876	3.436205
155.017246	3973.281464	6.703603	-0.031938	3.439481
155.101197	3981.336529	6.708608	-0.031959	3.442788
155.274015	3989.342636	6.713613	-0.031997	3.446074
155.454593	3997.391708	6.718618	-0.032036	3.449376
155.634178	4005.444081	6.723622	-0.032075	3.452675
155.891862	4013.473501	6.728627	-0.032129	3.455964
156.277790	4021.498109	6.733632	-0.032206	3.459253
156.496152	4029.489579	6.738637	-0.032253	3.462519
156.673493	4037.520348	6.743642	-0.032291	3.465797
157.065109	4045.551710	6.748646	-0.032370	3.469079
157.187349	4053.610746	6.753651	-0.032398	3.472360
157.543762	4061.639679	6.758656	-0.032470	3.475633
157.589909	4069.646260	6.763661	-0.032485	3.478884
157.878473	4077.658947	6.768666	-0.032544	3.482143
158.033949	4085.649666	6.773670	-0.032579	3.485385
158.098630	4093.675098	6.778675	-0.032596	3.488635
158.417731	4101.750694	6.783680	-0.032661	3.491911
158.579086	4109.741975	6.788685	-0.032697	3.495144
158.769404	4117.759376	6.793690	-0.032738	3.498386
158.854292	4125.804900	6.798694	-0.032760	3.501633
159.020112	4133.774129	6.803699	-0.032796	3.504849
159.257314	4141.828277	6.808704	-0.032846	3.508098
159.220142	4149.893314	6.813709	-0.032845	3.511340
159.716076	4157.906883	6.818714	-0.032943	3.514575
159.839031	4165.945031	6.823718	-0.032971	3.517805
159.870786	4173.968794	6.828723	-0.032983	3.521023
160.193005	4181.943432	6.833728	-0.033049	3.524228
160.091908	4189.993631	6.838733	-0.033035	3.527447
160.380424	4198.042627	6.843738	-0.033095	3.530674
160.417313	4206.093185	6.848742	-0.033107	3.533892
160.519847	4214.104668	6.853747	-0.033132	3.537093
160.661419	4222.149500	6.858752	-0.033164	3.540305
160.881265	4230.132325	6.863757	-0.033211	3.543493
161.228386	4238.189009	6.868762	-0.033281	3.546710
161.370951	4246.222930	6.873766	-0.033313	3.549910
161.318768	4254.343951	6.878771	-0.033309	3.553135
161.595822	4262.381739	6.883776	-0.033366	3.556334
161.845613	4270.289535	6.888781	-0.033419	3.559478
161.805330	4278.303954	6.893786	-0.033417	3.562653
161.836814	4286.334411	6.898790	-0.033428	3.565833
161.939055	4294.336054	6.903795	-0.033453	3.569001
162.206161	4302.394394	6.908800	-0.033508	3.572194
162.023274	4310.421851	6.913805	-0.033480	3.575358
162.472653	4318.398267	6.918810	-0.033569	3.578518
162.585428	4326.425494	6.923814	-0.033596	3.581685
162.761408	4334.403739	6.928819	-0.033634	3.584832
163.080634	4342.466019	6.933824	-0.033699	3.588014
163.058674	4350.514985	6.938829	-0.033701	3.591177
163.070804	4358.547118	6.943834	-0.033709	3.594332
163.493274	4366.558407	6.948838	-0.033793	3.597488
163.697207	4374.559142	6.953843	-0.033837	3.600631
163.922667	4382.562239	6.958848	-0.033884	3.603772
163.966547	4390.610118	6.963853	-0.033898	3.606923
164.117759	4398.606309	6.968858	-0.033932	3.610054
164.410954	4406.676993	6.973862	-0.033992	3.613215
164.274707	4414.710050	6.978867	-0.033973	3.616347
164.593966	4422.710677	6.983872	-0.034038	3.619477
164.874289	4430.742759	6.988877	-0.034096	3.622614
165.210939	4438.737075	6.993882	-0.034164	3.625736
165.274279	4446.786465	6.998886	-0.034181	3.628869
165.453183	4454.834787	7.003891	-0.034220	3.632002
165.772036	4462.891671	7.008896	-0.034285	3.635139
165.797067	4470.890717	7.013901	-0.034296	3.638243
166.052765	4478.918525	7.018906	-0.034349	3.641362
166.323976	4486.885337	7.023910	-0.034405	3.644455
166.261353	4494.946578	7.028915	-0.034399	3.647573
166.368766	4502.997379	7.033920	-0.034425	3.650689
166.653745	4511.009011	7.038925	-0.034484	3.653792
166.737808	4519.080943	7.043930	-0.034505	3.656909
166.734856	4527.054776	7.048934	-0.034510	3.659985
166.980010	4535.041190	7.053939	-0.034561	3.663069
167.290796	4543.134665	7.058944	-0.034625	3.666193
167.236648	4551.120956	7.063949	-0.034620	3.669264
167.419799	4559.168664	7.068954	-0.034660	3.672362
167.829574	4567.169027	7.073958	-0.034742	3.675444
167.955323	4575.168421	7.078963	-0.034771	3.678517
168.170461	4583.212603	7.083968	-0.034817	3.681607
168.229646	4591.198996	7.088973	-0.034834	3.684668
168.560375	4599.257308	7.093978	-0.034901	3.687760
168.499433	4607.249591	7.098982	-0.034895	3.690815
168.608936	4615.298555	7.103987	-0.034921	3.693893
168.950788	4623.337394	7.108992	-0.034991	3.696971
168.755288	4631.315932	7.113997	-0.034960	3.700010
168.921237	4639.364213	7.119002	-0.034996	3.703081
169.151365	4647.384736	7.124006	-0.035045	3.706142
169.208089	4655.389598	7.129011	-0.035061	3.709189
169.444242	4663.515156	7.134016	-0.035111	3.712284
169.574732	4671.548363	7.139021	-0.035141	3.715339
169.862782	4679.483485	7.144026	-0.035200	3.718358
170.028999	4687.507944	7.149030	-0.035237	3.721405
170.045936	4695.472777	7.154035	-0.035245	3.724424
170.551003	4703.519388	7.159040	-0.035345	3.727483
170.398604	4711.496558	7.164045	-0.035322	3.730497
170.479898	4719.595863	7.169050	-0.035343	3.733561
170.720932	4727.647951	7.174054	-0.035394	3.736608
170.805002	4735.586675	7.179059	-0.035415	3.739606
170.876195	4743.671771	7.184064	-0.035434	3.742657
170.901826	4751.667710	7.189069	-0.035444	3.745670
171.448898	4759.659153	7.194074	-0.035552	3.748691
171.569940	4767.738581	7.199078	-0.035580	3.751733
171.801601	4775.758773	7.204083	-0.035629	3.754753
171.978708	4783.770607	7.209088	-0.035667	3.757766
171.868601	4791.794162	7.214093	-0.035653	3.760775
172.049958	4799.830362	7.219098	-0.035692	3.763792
172.478178	4807.830480	7.224102	-0.035777	3.766799
172.622704	4815.831968	7.229107	-0.035810	3.769798
172.658932	4823.906603	7.234112	-0.035822	3.772819
172.779596	4831.929134	7.239117	-0.035851	3.775820
173.057796	4839.942736	7.244122	-0.035908	3.778819
173.341981	4847.964147	7.249126	-0.035967	3.781819
173.418716	4855.955090	7.254131	-0.035986	3.784800
173.749779	4864.007577	7.259136	-0.036054	3.787808
173.662656	4872.017727	7.264141	-0.036043	3.790788
173.744076	4880.099699	7.269146	-0.036064	3.793796
174.055102	4888.109819	7.274150	-0.036128	3.796780
174.259924	4896.058649	7.279155	-0.036171	3.799736
174.416663	4904.115071	7.284160	-0.036206	3.802729
174.326094	4912.098930	7.289165	-0.036195	3.805688
174.674093	4920.084396	7.294170	-0.036265	3.808654
174.960948	4928.170082	7.299174	-0.036325	3.811653
175.095719	4936.170631	7.304179	-0.036355	3.814616
175.064460	4944.256365	7.309184	-0.036355	3.817604
175.173234	4952.195747	7.314189	-0.036381	3.820539
175.513277	4960.231236	7.319194	-0.036450	3.823511
175.781849	4968.248434	7.324198	-0.036506	3.826474
175.789889	4976.247859	7.329203	-0.036513	3.829421
176.192942	4984.320043	7.334208	-0.036594	3.832402
176.349922	4992.315027	7.339213	-0.036628	3.835347
176.546872	5000.330962	7.344218	-0.036671	3.838298
176.658703	5008.351153	7.349222	-0.036697	3.841246
176.779287	5016.332825	7.354227	-0.036725	3.844178
176.979001	5024.401379	7.359232	-0.036768	3.847142
177.123947	5032.421351	7.364237	-0.036801	3.850084
177.274221	5040.479643	7.369242	-0.036834	3.853038
177.250994	5048.535019	7.374246	-0.036836	3.855985
177.457902	5056.501860	7.379251	-0.036880	3.858902
177.761782	5064.554978	7.384256	-0.036942	3.861851
177.964321	5072.519849	7.389261	-0.036986	3.864762
178.221364	5080.586303	7.394266	-0.037039	3.867710
178.161443	5088.612866	7.399270	-0.037034	3.870635
178.326917	5096.838200	7.404275	-0.037070	3.873634
178.441272	5104.844489	7.409280	-0.037097	3.876550
178.581699	5112.725790	7.414285	-0.037129	3.879420
178.730254	5120.713965	7.419290	-0.037162	3.882326
178.992494	5128.725346	7.424294	-0.037217	3.885240
179.060872	5136.716170	7.429299	-0.037235	3.888141
179.184585	5144.777250	7.434304	-0.037264	3.891066
179.102546	5152.816538	7.439309	-0.037254	3.893978
179.552444	5160.801898	7.444314	-0.037344	3.896877
179.701506	5168.791055	7.449318	-0.037377	3.899770
179.784237	5176.813007	7.454323	-0.037398	3.902672
179.977331	5184.845604	7.459328	-0.037440	3.905577
180.004333	5192.865199	7.464333	-0.037450	3.908473
180.180206	5200.877873	7.469338	-0.037489	3.911366
180.356141	5208.913892	7.474342	-0.037527	3.914266
180.590188	5216.914818	7.479347	-0.037576	3.917152
180.585834	5224.914838	7.484352	-0.037581	3.920031
180.513364	5232.945056	7.489357	-0.037573	3.922918
180.794684	5240.935419	7.494362	-0.037631	3.925794
181.041323	5248.980488	7.499366	-0.037683	3.928688
181.083831	5257.023592	7.504371	-0.037697	3.931575
181.285563	5265.062043	7.509376	-0.037740	3.934461
181.480818	5273.057129	7.514381	-0.037782	3.937329
181.786321	5281.028231	7.519386	-0.037844	3.940188
182.059941	5289.074055	7.524390	-0.037901	3.943072
182.078566	5297.069460	7.529395	-0.037910	3.945930
182.210285	5305.118450	7.534400	-0.037940	3.948808
182.294796	5313.174811	7.539405	-0.037962	3.951686
182.601676	5321.220121	7.544410	-0.038024	3.954561
182.934752	5329.240365	7.549414	-0.038092	3.957426
183.015569	5337.169170	7.554419	-0.038113	3.960252
183.228516	5345.221909	7.559424	-0.038158	3.963122
183.405305	5353.212074	7.564429	-0.038197	3.965967
183.277493	5361.219097	7.569434	-0.038178	3.968811
183.341219	5369.293049	7.574438	-0.038196	3.971679
183.537369	5377.309403	7.579443	-0.038238	3.974528
183.794056	5385.384219	7.584448	-0.038292	3.977396
183.802956	5393.343560	7.589453	-0.038299	3.980217
184.031309	5401.354728	7.594458	-0.038347	3.983058
184.189321	5409.361761	7.599462	-0.038382	3.985895
184.109445	5417.397094	7.604467	-0.038373	3.988735
184.309383	5425.495014	7.609472	-0.038416	3.991600
184.558065	5433.487821	7.614477	-0.038468	3.994427
184.743094	5441.492860	7.619482	-0.038508	3.997255
184.903818	5449.507421	7.624486	-0.038544	4.000083
184.979078	5457.519206	7.629491	-0.038563	4.002908
185.234049	5465.530332	7.634496	-0.038616	4.005733
185.284987	5473.522695	7.639501	-0.038631	4.008546
185.394435	5481.602453	7.644506	-0.038658	4.011389
185.453321	5489.674258	7.649510	-0.038674	4.014226
185.430711	5497.643362	7.654515	-0.038676	4.017024
185.710948	5505.628645	7.659520	-0.038733	4.019831
185.801458	5513.669858	7.664525	-0.038756	4.022652
186.053690	5521.677578	7.669530	-0.038809	4.025462
186.168955	5529.730885	7.674534	-0.038836	4.028283
186.492901	5537.746902	7.679539	-0.038902	4.031093
186.813876	5545.863463	7.684544	-0.038967	4.033936
186.861385	5553.862713	7.689549	-0.038982	4.036732
186.899743	5561.789219	7.694554	-0.038994	4.039500
187.096379	5569.816461	7.699558	-0.039037	4.042304
187.266637	5577.775252	7.704563	-0.039074	4.045082
187.423833	5585.843220	7.709568	-0.039109	4.047895
187.450074	5593.863195	7.714573	-0.039119	4.050688
187.746515	5601.871111	7.719578	-0.039180	4.053479
187.716573	5609.932432	7.724582	-0.039180	4.056281
187.743941	5617.899873	7.729587	-0.039191	4.059050
187.878165	5625.929515	7.734592	-0.039222	4.061840
188.197336	5633.910328	7.739597	-0.039287	4.064614
188.354173	5641.961026	7.744602	-0.039322	4.067408
188.672224	5649.977414	7.749606	-0.039387	4.070191
188.632583	5658.003119	7.754611	-0.039385	4.072969
188.851331	5666.082526	7.759616	-0.039431	4.075768
188.892934	5674.024783	7.764621	-0.039445	4.078515
189.262562	5682.043351	7.769626	-0.039519	4.081291
189.474515	5690.065676	7.774630	-0.039564	4.084064
189.513183	5698.083218	7.779635	-0.039577	4.086832
189.779875	5706.102667	7.784640	-0.039632	4.089601
189.865171	5714.166502	7.789645	-0.039654	4.092381
189.909708	5722.191205	7.794650	-0.039668	4.095145
190.163513	5730.202343	7.799654	-0.039721	4.097906
190.038492	5738.182777	7.804659	-0.039703	4.100649
190.377365	5746.193390	7.809664	-0.039772	4.103406
190.385794	5754.227633	7.814669	-0.039779	4.106166
190.663075	5762.230676	7.819674	-0.039836	4.108916
190.872650	5770.303684	7.824678	-0.039881	4.111688
191.044582	5778.345384	7.829683	-0.039919	4.114447
191.218963	5786.331381	7.834688	-0.039957	4.117184
191.560548	5794.278222	7.839693	-0.040026	4.119909
191.686563	5802.325198	7.844698	-0.040055	4.122663
192.053123	5810.329461	7.849702	-0.040129	4.125404
192.029064	5818.379133	7.854707	-0.040130	4.128154
192.202809	5826.419634	7.859712	-0.040168	4.130901
192.214217	5834.448574	7.864717	-0.040176	4.133640
192.588776	5842.457835	7.869722	-0.040252	4.136375
192.888977	5850.491730	7.874726	-0.040313	4.139116
192.746547	5858.521204	7.879731	-0.040292	4.141848
193.274364	5866.478889	7.884736	-0.040396	4.144562
193.293389	5874.561939	7.889741	-0.040405	4.147311
193.394233	5882.532604	7.894746	-0.040430	4.150020
193.567381	5890.616369	7.899750	-0.040468	4.152767
193.696143	5898.634403	7.904755	-0.040497	4.155490
193.972737	5906.631468	7.909760	-0.040555	4.158205
193.859734	5914.614088	7.914765	-0.040539	4.160909
194.106056	5922.584980	7.919770	-0.040591	4.163611
194.293791	5930.670188	7.924774	-0.040631	4.166350
194.333907	5938.663293	7.929779	-0.040644	4.169054
194.617359	5946.721817	7.934784	-0.040703	4.171781
194.709750	5954.742188	7.939789	-0.040726	4.174491
194.812704	5962.746189	7.944794	-0.040751	4.177194
195.218442	5970.747289	7.949798	-0.040832	4.179898
195.253136	5978.762205	7.954803	-0.040844	4.182600
195.402787	5986.762822	7.959808	-0.040877	4.185297
195.372942	5994.804166	7.964813	-0.040877	4.188004
195.868220	6002.799457	7.969818	-0.040975	4.190700
195.974678	6010.924936	7.974822	-0.041001	4.193433
196.215616	6018.944610	7.979827	-0.041051	4.196131
196.461194	6026.888495	7.984832	-0.041103	4.198801
196.490591	6034.889937	7.989837	-0.041114	4.201486
196.496835	6042.859994	7.994842	-0.041121	4.204159
196.587082	6050.931297	7.999846	-0.041143	4.206866
196.773825	6058.888317	8.004851	-0.041183	4.209533
196.972414	6066.978858	8.009856	-0.041226	4.212243
197.096736	6074.985469	8.014861	-0.041255	4.214923
197.359153	6082.953819	8.019866	-0.041309	4.217589
197.590612	6090.979672	8.024870	-0.041358	4.220273
197.506057	6098.970599	8.029875	-0.041348	4.222940
197.759010	6107.022991	8.034880	-0.041401	4.225629
197.836441	6115.051145	8.039885	-0.041421	4.228307
197.961356	6123.053049	8.044890	-0.041450	4.230975
198.347149	6131.101238	8.049894	-0.041527	4.233659
198.477900	6139.142363	8.054899	-0.041557	4.236336
198.596807	6147.124188	8.059904	-0.041585	4.238992
198.845116	6155.133695	8.064909	-0.041637	4.241657
198.866223	6163.108712	8.069914	-0.041647	4.244306
199.057560	6171.190247	8.074918	-0.041688	4.246990
199.033674	6179.153086	8.079923	-0.041689	4.249632
199.057500	6187.257077	8.084928	-0.041699	4.252319
199.306126	6195.273310	8.089933	-0.041751	4.254978
199.645883	6203.293119	8.094938	-0.041820	4.257636
199.657221	6211.319450	8.099942	-0.041828	4.260292
199.841790	6219.291366	8.104947	-0.041868	4.262930
200.068797	6227.264332	8.109952	-0.041916	4.265568
200.151855	6235.338815	8.114957	-0.041937	4.268235
200.309724	6243.341678	8.119962	-0.041972	4.270878
200.695402	6251.467626	8.124966	-0.042049	4.273562
200.827066	6259.442512	8.129971	-0.042080	4.276193
201.108374	6267.440314	8.134976	-0.042138	4.278830
201.320192	6275.456331	8.139981	-0.042183	4.281471
201.487097	6283.422539	8.144986	-0.042219	4.284094
201.668313	6291.506351	8.149990	-0.042259	4.286754
201.756869	6299.432242	8.154995	-0.042281	4.289360
202.016700	6307.547960	8.160000	-0.042335	4.292028
201.998007	6315.524421	8.165005	-0.042337	4.294646
202.310910	6323.551919	8.170010	-0.042401	4.297282
202.514075	6331.525220	8.175014	-0.042445	4.299897
202.545955	6339.573349	8.180019	-0.042456	4.302534
202.933987	6347.588385	8.185024	-0.042534	4.305162
203.165462	6355.616954	8.190029	-0.042583	4.307791
203.346801	6363.613508	8.195034	-0.042622	4.310407
203.384413	6371.708161	8.200038	-0.042635	4.313053
203.519677	6379.657362	8.205043	-0.042666	4.315651
203.777539	6387.699497	8.210048	-0.042719	4.318278
203.649029	6395.674030	8.215053	-0.042701	4.320879
203.814441	6403.640015	8.220058	-0.042738	4.323477
204.132212	6411.713860	8.225062	-0.042802	4.326110
204.247446	6419.689821	8.230067	-0.042830	4.328708
204.325120	6427.798119	8.235072	-0.042850	4.331348
204.603339	6435.810075	8.240077	-0.042907	4.333955
204.534775	6443.805605	8.245082	-0.042900	4.336554
204.710451	6451.795904	8.250086	-0.042938	4.339151
204.906319	6459.832967	8.255091	-0.042980	4.341761
205.326338	6467.788455	8.260096	-0.043064	4.344345
205.224779	6475.869452	8.265101	-0.043051	4.346965
205.271121	6483.887691	8.270106	-0.043065	4.349564
205.472941	6491.930735	8.275110	-0.043109	4.352170
205.564218	6499.992492	8.280115	-0.043131	4.354780
205.594145	6508.007256	8.285120	-0.043143	4.357373
205.846563	6515.943211	8.290125	-0.043195	4.359940
206.146323	6523.945854	8.295130	-0.043257	4.362528
206.389645	6531.950600	8.300134	-0.043308	4.365114
206.367210	6539.977871	8.305139	-0.043309	4.367704
206.491279	6548.011970	8.310144	-0.043338	4.370296
206.552998	6556.045285	8.315149	-0.043355	4.372886
206.611474	6564.069883	8.320154	-0.043371	4.375471
206.893916	6572.095143	8.325158	-0.043430	4.378057
206.979722	6580.065754	8.330163	-0.043451	4.380622
207.088783	6588.068825	8.335168	-0.043477	4.383196
207.157881	6596.089997	8.340173	-0.043496	4.385774
207.312713	6604.099830	8.345178	-0.043530	4.388347
207.480767	6612.149230	8.350182	-0.043567	4.390932
207.741880	6620.130783	8.355187	-0.043622	4.393494
208.010881	6628.224120	8.360192	-0.043677	4.396090
208.079627	6636.165885	8.365197	-0.043696	4.398635
208.040128	6644.196002	8.370202	-0.043694	4.401206
208.444830	6652.201066	8.375206	-0.043775	4.403771
208.477714	6660.239459	8.380211	-0.043787	4.406342
208.586835	6668.262784	8.385216	-0.043813	4.408907
208.731218	6676.308847	8.390221	-0.043845	4.411479
208.825053	6684.305691	8.395226	-0.043868	4.414032
208.953079	6692.354636	8.400230	-0.043898	4.416601
208.996503	6700.315614	8.405235	-0.043912	4.419141
209.301607	6708.400706	8.410240	-0.043974	4.421719
209.547701	6716.354274	8.415245	-0.044026	4.424254
209.555358	6724.384675	8.420250	-0.044033	4.426810
209.732900	6732.432973	8.425254	-0.044071	4.429372
209.738762	6740.474714	8.430259	-0.044078	4.431929
209.989696	6748.490142	8.435264	-0.044131	4.434478
209.983767	6756.547289	8.440269	-0.044135	4.437037
210.255950	6764.464601	8.445274	-0.044191	4.439551
210.561532	6772.555375	8.450278	-0.044254	4.442119
210.642401	6780.461893	8.455283	-0.044275	4.444627
210.599954	6788.555862	8.460288	-0.044272	4.447191
210.705831	6796.562848	8.465293	-0.044298	4.449728
210.909325	6804.591955	8.470298	-0.044341	4.452270
211.248208	6812.622069	8.475302	-0.044410	4.454812
211.240641	6820.645384	8.480307	-0.044414	4.457348
211.353505	6828.579898	8.485312	-0.044441	4.459856
211.443434	6836.667537	8.490317	-0.044463	4.462410
211.540111	6844.608389	8.495322	-0.044487	4.464917
212.003894	6852.709886	8.500326	-0.044579	4.467474
212.098558	6860.656968	8.505331	-0.044602	4.469980
212.403687	6868.749920	8.510336	-0.044665	4.472531
212.444422	6876.768212	8.515341	-0.044678	4.475056
212.528572	6884.762806	8.520346	-0.044699	4.477572
212.959380	6892.749331	8.525350	-0.044785	4.480086
212.798839	6900.773490	8.530355	-0.044761	4.482608
212.969022	6908.716239	8.535360	-0.044798	4.485104
213.156247	6916.752825	8.540365	-0.044839	4.487628
213.547742	6924.781069	8.545370	-0.044917	4.490149
213.622517	6932.856859	8.550374	-0.044937	4.492682
213.600964	6940.864433	8.555379	-0.044939	4.495192
213.847122	6948.867034	8.560384	-0.044990	4.497700
213.944391	6956.863585	8.565389	-0.045014	4.500204
213.871393	6964.861152	8.570394	-0.045006	4.502707
214.088009	6972.898586	8.575399	-0.045052	4.505221
214.234208	6980.912228	8.580403	-0.045085	4.507726
214.523365	6988.935211	8.585408	-0.045144	4.510234
214.672198	6997.004919	8.590413	-0.045178	4.512754
214.816570	7004.994180	8.595418	-0.045210	4.515247
214.930541	7013.054239	8.600423	-0.045237	4.517761
214.973833	7020.978113	8.605427	-0.045251	4.520232
215.211875	7028.994139	8.610432	-0.045301	4.522730
215.414231	7037.003920	8.615437	-0.045344	4.525224
215.464280	7045.018255	8.620442	-0.045359	4.527718
215.601316	7053.015369	8.625447	-0.045390	4.530206
215.597326	7061.034937	8.630451	-0.045395	4.532699
215.947203	7069.104942	8.635456	-0.045466	4.535207
215.997530	7077.084843	8.640461	-0.045481	4.537685
216.419942	7085.037749	8.645466	-0.045565	4.540153
216.456222	7093.116174	8.650471	-0.045578	4.542659
216.509243	7101.112355	8.655475	-0.045593	4.545138
216.785581	7109.160120	8.660480	-0.045650	4.547632
216.945488	7117.164611	8.665485	-0.045686	4.550111
216.875346	7125.206965	8.670490	-0.045678	4.552600
217.117693	7133.280486	8.675495	-0.045729	4.555097
217.194360	7141.257270	8.680499	-0.045749	4.557563
217.454538	7149.184044	8.685504	-0.045803	4.560013
217.723035	7157.278982	8.690509	-0.045859	4.562513
217.671485	7165.211781	8.695514	-0.045855	4.564961
218.073294	7173.317194	8.700519	-0.045935	4.567462
218.060951	7181.275745	8.705523	-0.045939	4.569915
218.105355	7189.383313	8.710528	-0.045953	4.572414
218.464770	7197.408143	8.715533	-0.046025	4.574885
218.639062	7205.404534	8.720538	-0.046063	4.577347
218.629992	7213.356078	8.725543	-0.046067	4.579793
218.805087	7221.414999	8.730547	-0.046106	4.582271
218.951393	7229.398144	8.735552	-0.046138	4.584724
219.214225	7237.457566	8.740557	-0.046193	4.587200
219.053445	7245.444991	8.745562	-0.046169	4.589651
219.380149	7253.541602	8.750567	-0.046235	4.592135
219.530473	7261.499421	8.755571	-0.046269	4.594576
219.548785	7269.532038	8.760576	-0.046278	4.597037
219.774026	7277.477979	8.765581	-0.046325	4.599471
219.831687	7285.540611	8.770586	-0.046342	4.601939
219.978705	7293.507503	8.775591	-0.046375	4.604377
220.174826	7301.524604	8.780595	-0.046417	4.606829
220.544522	7309.538828	8.785600	-0.046492	4.609278
220.615245	7317.627065	8.790605	-0.046510	4.611749
220.518005	7325.619450	8.795610	-0.046498	4.614189
220.801343	7333.673391	8.800615	-0.046556	4.616647
220.773285	7341.623109	8.805619	-0.046557	4.619071
221.029949	7349.685740	8.810624	-0.046610	4.621529
221.364003	7357.665699	8.815629	-0.046678	4.623960
221.520557	7365.700089	8.820634	-0.046713	4.626407
221.617968	7373.700770	8.825639	-0.046737	4.628841
221.716075	7381.757045	8.830643	-0.046761	4.631292
222.025827	7389.771723	8.835648	-0.046824	4.633728
222.170312	7397.803832	8.840653	-0.046857	4.636169
222.249551	7405.734200	8.845658	-0.046877	4.638577
222.324722	7413.794239	8.850663	-0.046897	4.641023
222.474709	7421.766094	8.855667	-0.046930	4.643442
222.542229	7429.766686	8.860672	-0.046948	4.645868
222.857185	7437.828826	8.865677	-0.047013	4.648311
222.724421	7445.813646	8.870682	-0.046994	4.650729
223.047391	7453.891647	8.875687	-0.047059	4.653174
223.081754	7461.903946	8.880691	-0.047071	4.655599
223.280913	7469.906552	8.885696	-0.047114	4.658018
223.288003	7477.911676	8.890701	-0.047121	4.660438
223.471375	7485.918544	8.895706	-0.047161	4.662857
223.983103	7493.937171	8.900711	-0.047262	4.665277
224.116968	7501.949267	8.905715	-0.047292	4.667695
223.901372	7509.924695	8.910720	-0.047258	4.670101
224.194656	7518.078458	8.915725	-0.047318	4.672558
224.190038	7526.090108	8.920730	-0.047323	4.674972
224.272266	7534.057601	8.925735	-0.047344	4.677371
224.472254	7542.002859	8.930739	-0.047387	4.679763
224.857380	7550.069524	8.935744	-0.047464	4.682189
224.829790	7557.998021	8.940749	-0.047465	4.684573
224.676759	7566.054527	8.945754	-0.047442	4.686994
225.099207	7574.071792	8.950759	-0.047526	4.689401
225.245579	7582.088530	8.955763	-0.047559	4.691808
225.490978	7590.098630	8.960768	-0.047610	4.694211
225.587179	7598.175479	8.965773	-0.047634	4.696633
225.697448	7606.043066	8.970778	-0.047660	4.698991
226.131894	7614.143092	8.975783	-0.047747	4.701417
226.139025	7622.166215	8.980787	-0.047754	4.703819
226.373775	7630.209727	8.985792	-0.047803	4.706226
226.264852	7638.194321	8.990797	-0.047788	4.708615
226.266162	7646.181697	8.995802	-0.047794	4.711003
226.601350	7654.309541	9.000807	-0.047862	4.713431
226.983605	7662.238207	9.005811	-0.047939	4.715798
226.959521	7670.295266	9.010816	-0.047940	4.718203
227.218685	7678.264643	9.015821	-0.047994	4.720580
227.391804	7686.311747	9.020826	-0.048032	4.722979
227.424973	7694.358633	9.025831	-0.048044	4.725377
227.331747	7702.371792	9.030835	-0.048032	4.727765
227.549784	7710.355153	9.035840	-0.048079	4.730141
227.809653	7718.430111	9.040845	-0.048133	4.732544
227.851635	7726.399040	9.045850	-0.048146	4.734914
227.968554	7734.439951	9.050855	-0.048174	4.737304
228.393583	7742.393489	9.055859	-0.048258	4.739666
228.336979	7750.445070	9.060864	-0.048253	4.742058
228.564605	7758.480525	9.065869	-0.048301	4.744442
228.514181	7766.450854	9.070874	-0.048298	4.746807
228.766384	7774.477917	9.075879	-0.048350	4.749187
228.674975	7782.481091	9.080883	-0.048339	4.751559
229.196913	7790.561529	9.085888	-0.048442	4.753951
229.108156	7798.592871	9.090893	-0.048431	4.756330
229.123017	7806.533390	9.095898	-0.048439	4.758680
229.600717	7814.558265	9.100903	-0.048534	4.761052
229.691367	7822.552060	9.105907	-0.048556	4.763415
229.829379	7830.554672	9.110912	-0.048588	4.765779
229.881265	7838.605717	9.115917	-0.048603	4.768157
230.004153	7846.580250	9.120922	-0.048632	4.770510
230.186219	7854.661135	9.125927	-0.048671	4.772894
230.171995	7862.677941	9.130931	-0.048674	4.775258
230.346462	7870.676841	9.135936	-0.048712	4.777615
230.617631	7878.719218	9.140941	-0.048769	4.779984
230.668657	7886.656664	9.145946	-0.048784	4.782321
230.726774	7894.671326	9.150951	-0.048800	4.784680
230.907150	7902.703357	9.155955	-0.048839	4.787042
231.075215	7910.735009	9.160960	-0.048876	4.789403
231.316126	7918.732427	9.165965	-0.048927	4.791752
231.460274	7926.770737	9.170970	-0.048959	4.794112
231.554099	7934.815522	9.175975	-0.048982	4.796474
231.713711	7942.776972	9.180979	-0.049018	4.798809
231.859617	7950.807109	9.185984	-0.049051	4.801164
232.134282	7958.838963	9.190989	-0.049107	4.803517
232.118613	7966.796833	9.195994	-0.049110	4.805849
232.483611	7974.873304	9.200999	-0.049184	4.808213
232.601343	7982.839022	9.206003	-0.049211	4.810544
232.600652	7990.260296	9.211008	-0.049216	4.812716
232.858433	7994.814947	9.216013	-0.049268	4.814046

232.984426	7997.329244	9.221018	-0.049293	4.814781
233.259101	7998.591609	9.226023	-0.049346	4.815149
232.920316	7999.000454	9.231027	-0.049283	4.815270
233.095228	8000.045606	9.236032	-0.049317	4.815575
233.435616	8000.077895	9.241037	-0.049381	4.815582
233.494595	8000.061807	9.246042	-0.049392	4.815577
233.591484	8000.090124	9.251047	-0.049411	4.815585
233.602960	8000.075398	9.256051	-0.049413	4.815581
233.790648	8000.090246	9.261056	-0.049449	4.815584
233.828856	8000.072752	9.266061	-0.049456	4.815579
233.690987	8000.054520	9.271066	-0.049431	4.815574
234.011444	8000.100370	9.276071	-0.049491	4.815586
233.926175	8000.069113	9.281075	-0.049476	4.815577
233.936016	8000.094942	9.286080	-0.049478	4.815585
234.016488	8000.120856	9.291085	-0.049493	4.815592
233.971382	8000.074235	9.296090	-0.049485	4.815579
234.110841	8000.125675	9.301095	-0.049512	4.815593
234.119365	8000.101288	9.306099	-0.049514	4.815586
234.210296	8000.110286	9.311104	-0.049531	4.815588
234.185710	8000.129146	9.316109	-0.049527	4.815594
234.018434	8000.084803	9.321114	-0.049496	4.815582
234.246955	8000.147308	9.326119	-0.049539	4.815599
234.111227	8000.123771	9.331123	-0.049514	4.815592
233.982382	8000.102482	9.336128	-0.049491	4.815587
234.206681	8000.143559	9.341133	-0.049533	4.815598
234.350029	8000.109626	9.346138	-0.049560	4.815587
234.320327	8000.123062	9.351143	-0.049555	4.815591
234.292819	8000.108767	9.356147	-0.049550	4.815587
234.490161	8000.104550	9.361152	-0.049588	4.815585
234.391835	8000.121138	9.366157	-0.049570	4.815590
234.309426	8000.081384	9.371162	-0.049555	4.815579
234.255781	8000.139284	9.376167	-0.049545	4.815596
234.183180	8000.103962	9.381171	-0.049532	4.815586
234.081598	8000.092730	9.386176	-0.049514	4.815583
234.414258	8000.117421	9.391181	-0.049576	4.815589
234.199472	8000.084049	9.396186	-0.049536	4.815580
234.564913	8000.159470	9.401191	-0.049605	4.815601
234.542662	8000.095066	9.406195	-0.049601	4.815582
234.526602	8000.103385	9.411200	-0.049599	4.815584
234.474678	8000.126071	9.416205	-0.049589	4.815591
234.170613	8000.106193	9.421210	-0.049533	4.815587
234.368465	8000.136160	9.426215	-0.049571	4.815595
234.694251	8000.119088	9.431219	-0.049632	4.815588
234.414115	8000.118825	9.436224	-0.049580	4.815589
234.543489	8000.140198	9.441229	-0.049604	4.815595
234.433119	8000.139502	9.446234	-0.049584	4.815595
234.593210	8000.149628	9.451239	-0.049615	4.815597
234.702565	8000.134364	9.456243	-0.049635	4.815592
234.534646	8000.131660	9.461248	-0.049604	4.815592
234.829452	8000.133307	9.466253	-0.049660	4.815592
234.633857	8000.140831	9.471258	-0.049624	4.815595
234.678173	8000.137320	9.476263	-0.049632	4.815593
234.519276	8000.116608	9.481267	-0.049603	4.815588
234.560762	8000.128002	9.486272	-0.049611	4.815591
234.696120	8000.206076	9.491277	-0.049637	4.815613
234.800104	8000.138393	9.496282	-0.049657	4.815593
234.732201	8000.160818	9.501287	-0.049645	4.815600
234.606895	8000.138518	9.506291	-0.049622	4.815594
234.835547	8000.126269	9.511296	-0.049665	4.815589
234.789896	8000.160804	9.516301	-0.049657	4.815600
234.806910	8000.120537	9.521306	-0.049660	4.815588
234.814147	8000.171955	9.526311	-0.049662	4.815603
234.708759	8000.177748	9.531315	-0.049643	4.815605
234.732974	8000.108763	9.536320	-0.049648	4.815585
234.818542	8000.167868	9.541325	-0.049664	4.815601
234.846036	8000.112820	9.546330	-0.049670	4.815585
234.918712	8000.225114	9.551335	-0.049684	4.815618
234.832721	8000.153261	9.556339	-0.049668	4.815597
234.921058	8000.169693	9.561344	-0.049685	4.815601
235.045660	8000.221960	9.566349	-0.049709	4.815616
234.926885	8000.130348	9.571354	-0.049687	4.815590
234.885058	8000.127566	9.576359	-0.049680	4.815589
234.895876	8000.188656	9.581363	-0.049682	4.815607
234.930521	8000.133724	9.586368	-0.049689	4.815591
235.104037	8000.193198	9.591373	-0.049722	4.815607
234.880377	8000.135116	9.596378	-0.049680	4.815592
234.884051	8000.156573	9.601383	-0.049682	4.815598
234.856216	8000.138001	9.606387	-0.049677	4.815592
235.067675	8000.120131	9.611392	-0.049717	4.815586
235.264502	8000.158627	9.616397	-0.049754	4.815596
234.943226	8000.123515	9.621402	-0.049694	4.815588
234.917199	8000.134875	9.626407	-0.049690	4.815591
234.963667	8000.145283	9.631411	-0.049699	4.815594
234.819852	8000.134429	9.636416	-0.049673	4.815592
234.839506	8000.178575	9.641421	-0.049677	4.815604
234.974324	8000.178678	9.646426	-0.049702	4.815604
235.040480	8000.170184	9.651431	-0.049715	4.815601
235.042851	8000.152104	9.656435	-0.049716	4.815596
235.160290	8000.185031	9.661440	-0.049738	4.815605
235.312642	8000.250569	9.666445	-0.049767	4.815623
235.125205	8000.157834	9.671450	-0.049732	4.815597
235.074142	8000.159174	9.676455	-0.049723	4.815597
235.184317	8000.186642	9.681459	-0.049744	4.815605
235.117071	8000.133250	9.686464	-0.049732	4.815590
235.175020	8000.141710	9.691469	-0.049743	4.815592
235.197784	8000.135711	9.696474	-0.049748	4.815590
235.045410	8000.137533	9.701479	-0.049720	4.815591
235.084572	8000.139278	9.706483	-0.049728	4.815592
235.204548	8000.135935	9.711488	-0.049751	4.815590
235.322971	8000.157130	9.716493	-0.049773	4.815596
234.968616	8000.096914	9.721498	-0.049708	4.815580
235.156951	8000.158766	9.726503	-0.049743	4.815597
235.289700	8000.166312	9.731507	-0.049768	4.815598
235.281596	8000.139517	9.736512	-0.049767	4.815591
235.230121	8000.183570	9.741517	-0.049758	4.815604
234.983446	8000.159287	9.746522	-0.049712	4.815598
235.197424	8000.162819	9.751527	-0.049753	4.815598
235.089760	8000.130127	9.756531	-0.049733	4.815589
235.169955	8000.145358	9.761536	-0.049748	4.815593
235.313994	8000.168040	9.766541	-0.049776	4.815599
235.327858	8000.144808	9.771546	-0.049779	4.815592
235.242496	8000.185103	9.776551	-0.049763	4.815604
235.069370	8000.135322	9.781555	-0.049731	4.815590
235.365920	8000.132726	9.786560	-0.049787	4.815588
235.380829	8000.177863	9.791565	-0.049790	4.815601
235.125452	8000.117127	9.796570	-0.049743	4.815585
235.393167	8000.149304	9.801575	-0.049793	4.815593
235.129206	8000.101243	9.806579	-0.049745	4.815580
235.172283	8000.152180	9.811584	-0.049753	4.815595
235.311686	8000.167310	9.816589	-0.049780	4.815598
235.181389	8000.156676	9.821594	-0.049756	4.815596
235.340930	8000.204175	9.826599	-0.049786	4.815609
235.230213	8000.183180	9.831603	-0.049766	4.815603
235.380442	8000.144020	9.836608	-0.049794	4.815591
235.527083	8000.172085	9.841613	-0.049822	4.815599
235.504305	8000.205926	9.846618	-0.049818	4.815609
235.298890	8000.204745	9.851623	-0.049780	4.815609
235.257639	8000.201972	9.856627	-0.049773	4.815609
235.234364	8000.198426	9.861632	-0.049769	4.815608
235.528081	8000.219281	9.866637	-0.049824	4.815612
235.284246	8000.221744	9.871642	-0.049779	4.815614
235.265158	8000.189430	9.876647	-0.049776	4.815605
235.232916	8000.202825	9.881651	-0.049771	4.815609
235.553353	8000.171784	9.886656	-0.049831	4.815598
235.583171	8000.186193	9.891661	-0.049837	4.815602
235.272808	8000.139509	9.896666	-0.049779	4.815590
235.243488	8000.186060	9.901671	-0.049774	4.815604
235.332095	8000.148029	9.906675	-0.049791	4.815592
235.528746	8000.161958	9.911680	-0.049828	4.815596
235.657857	8000.183329	9.916685	-0.049853	4.815601
235.591764	8000.182287	9.921690	-0.049841	4.815601
235.396772	8000.167392	9.926695	-0.049805	4.815598
235.416904	8000.157078	9.931699	-0.049809	4.815595
235.426917	8000.171163	9.936704	-0.049811	4.815599
235.354021	8000.167874	9.941709	-0.049798	4.815598
235.388876	8000.157801	9.946714	-0.049805	4.815595
235.528754	8000.186824	9.951719	-0.049832	4.815603
235.457134	8000.178215	9.956723	-0.049819	4.815601
235.415932	8000.183988	9.961728	-0.049811	4.815602
235.545533	8000.200027	9.966733	-0.049836	4.815606
235.761913	8000.130974	9.971738	-0.049877	4.815585
235.513783	8000.155795	9.976743	-0.049831	4.815594
235.423769	8000.162906	9.981747	-0.049815	4.815596
235.500142	8000.184484	9.986752	-0.049829	4.815602
235.649619	8000.158127	9.991757	-0.049858	4.815594
235.477736	8000.150017	9.996762	-0.049826	4.815592
235.642199	8000.191189	10.001767	-0.049857	4.815603
235.543240	8000.201358	10.006771	-0.049839	4.815607
235.744082	8000.185453	10.011776	-0.049877	4.815601
236.002269	8000.207865	10.016781	-0.049925	4.815606
235.810143	8000.167383	10.021786	-0.049890	4.815596
235.815194	8000.236924	10.026791	-0.049891	4.815616
235.835210	8000.222336	10.031795	-0.049896	4.815611
235.735821	8000.145989	10.036800	-0.049877	4.815590
235.678351	8000.226257	10.041805	-0.049867	4.815613
235.466394	8000.215356	10.046810	-0.049828	4.815611
235.767293	8000.205357	10.051815	-0.049885	4.815607
235.673963	8000.209210	10.056819	-0.049868	4.815608
235.564141	8000.172209	10.061824	-0.049848	4.815598
235.713465	8000.204591	10.066829	-0.049876	4.815607
235.789254	8000.228295	10.071834	-0.049890	4.815613
235.786906	8000.181301	10.076839	-0.049890	4.815600
235.586682	8000.223993	10.081843	-0.049854	4.815613
235.611735	8000.207351	10.086848	-0.049859	4.815608
236.004233	8000.224482	10.091853	-0.049932	4.815611
235.679750	8000.132709	10.096858	-0.049872	4.815586
235.869641	8000.154005	10.101863	-0.049908	4.815591
235.768367	8000.219673	10.106867	-0.049890	4.815611
235.653761	8000.164438	10.111872	-0.049869	4.815595
235.778651	8000.239140	10.116877	-0.049892	4.815616
235.862060	8000.226657	10.121882	-0.049908	4.815612
235.603319	8000.206447	10.126887	-0.049861	4.815608
235.754481	8000.252743	10.131891	-0.049889	4.815621
235.632780	8000.158943	10.136896	-0.049867	4.815594
235.722727	8000.194626	10.141901	-0.049884	4.815604
235.674882	8000.226991	10.146906	-0.049876	4.815613
235.871196	8000.217419	10.151911	-0.049913	4.815610
235.745299	8000.259189	10.156915	-0.049890	4.815622
235.871656	8000.161965	10.161920	-0.049913	4.815593
235.555799	8000.195291	10.166925	-0.049855	4.815605
235.686078	8000.234838	10.171930	-0.049880	4.815616
235.816693	8000.185745	10.176935	-0.049905	4.815601
235.765911	8000.256510	10.181939	-0.049896	4.815621
235.816615	8000.186887	10.186944	-0.049905	4.815601
235.898475	8000.197874	10.191949	-0.049921	4.815604
235.758529	8000.136884	10.196954	-0.049895	4.815587
235.641716	8000.195890	10.201959	-0.049874	4.815604
235.769506	8000.198016	10.206963	-0.049898	4.815604
235.655855	8000.206877	10.211968	-0.049878	4.815607
235.794566	8000.262582	10.216973	-0.049904	4.815623
235.776548	8000.186495	10.221978	-0.049901	4.815601
235.758298	8000.184099	10.226983	-0.049898	4.815600
235.884097	8000.260953	10.231987	-0.049922	4.815622
235.813195	8000.189343	10.236992	-0.049909	4.815601
235.866403	8000.250059	10.241997	-0.049919	4.815619
235.798769	8000.218019	10.247002	-0.049907	4.815610
235.849970	8000.185785	10.252007	-0.049917	4.815600
236.170057	8000.210277	10.257011	-0.049977	4.815606
236.010183	8000.154301	10.262016	-0.049948	4.815590
236.026064	8000.175959	10.267021	-0.049951	4.815596
235.911238	8000.191208	10.272026	-0.049930	4.815601
235.910806	8000.232892	10.277031	-0.049931	4.815614
236.041814	8000.206233	10.282035	-0.049955	4.815605
235.900660	8000.176196	10.287040	-0.049930	4.815597
236.037013	8000.239339	10.292045	-0.049955	4.815615
235.978338	8000.199969	10.297050	-0.049945	4.815604
236.015457	8000.201681	10.302055	-0.049952	4.815604
235.968058	8000.249005	10.307059	-0.049944	4.815618
235.815179	8000.208096	10.312064	-0.049916	4.815607
235.754026	8000.270148	10.317069	-0.049905	4.815625
235.871176	8000.228311	10.322074	-0.049927	4.815612
235.913823	8000.215161	10.327079	-0.049936	4.815608
235.781621	8000.187406	10.332083	-0.049911	4.815601
235.829813	8000.146579	10.337088	-0.049921	4.815589
236.042976	8000.233405	10.342093	-0.049961	4.815613
235.958695	8000.189344	10.347098	-0.049946	4.815601
235.962080	8000.218274	10.352103	-0.049947	4.815609
236.107620	8000.208941	10.357107	-0.049974	4.815606
236.066658	8000.183745	10.362112	-0.049967	4.815598
236.195275	8000.286279	10.367117	-0.049991	4.815628
236.050802	8000.201718	10.372122	-0.049965	4.815604
236.046369	8000.233724	10.377127	-0.049964	4.815613
235.799043	8000.200883	10.382131	-0.049919	4.815605
235.925777	8000.182699	10.387136	-0.049943	4.815599
236.082975	8000.203462	10.392141	-0.049973	4.815604
236.170527	8000.175026	10.397146	-0.049989	4.815595
235.967972	8000.240107	10.402151	-0.049952	4.815615
235.957817	8000.252795	10.407155	-0.049951	4.815619
235.866964	8000.170178	10.412160	-0.049934	4.815595
236.144746	8000.222816	10.417165	-0.049986	4.815609
236.158479	8000.192105	10.422170	-0.049989	4.815600
236.046044	8000.212734	10.427175	-0.049969	4.815607
235.934713	8000.232313	10.432179	-0.049948	4.815613
235.868231	8000.177863	10.437184	-0.049936	4.815597
236.109779	8000.216025	10.442189	-0.049982	4.815607
236.030379	8000.214765	10.447194	-0.049968	4.815607
235.976584	8000.188291	10.452199	-0.049958	4.815600
236.082728	8000.207151	10.457203	-0.049978	4.815605
236.079661	8000.170826	10.462208	-0.049978	4.815594
236.006903	8000.232688	10.467213	-0.049965	4.815613
236.064051	8000.178122	10.472218	-0.049976	4.815596
236.263666	8000.183558	10.477223	-0.050014	4.815597
236.076746	8000.242487	10.482227	-0.049979	4.815615
235.929589	8000.205943	10.487232	-0.049952	4.815605
235.979429	8000.240972	10.492237	-0.049962	4.815615
236.044503	8000.159835	10.497242	-0.049974	4.815591
236.003687	8000.182702	10.502247	-0.049967	4.815598
236.043707	8000.328645	10.507251	-0.049975	4.815641
236.136876	8000.222335	10.512256	-0.049993	4.815609
236.154224	8000.296350	10.517261	-0.049997	4.815631
235.892972	8000.230173	10.522266	-0.049948	4.815612
236.061218	8000.193442	10.527271	-0.049980	4.815601
236.070295	8000.205377	10.532275	-0.049982	4.815604
235.984027	8000.182644	10.537280	-0.049967	4.815598
236.113078	8000.213627	10.542285	-0.049991	4.815606
236.034808	8000.233746	10.547290	-0.049977	4.815613
236.043403	8000.211496	10.552295	-0.049979	4.815606
236.081237	8000.293322	10.557299	-0.049986	4.815630
236.005238	8000.233376	10.562304	-0.049973	4.815613
236.177005	8000.223404	10.567309	-0.050005	4.815609
235.939611	8000.182182	10.572314	-0.049961	4.815598
236.191911	8000.179934	10.577319	-0.050009	4.815596
236.178594	8000.257720	10.582323	-0.050007	4.815619
236.083512	8000.163286	10.587328	-0.049989	4.815592
236.271335	8000.319121	10.592333	-0.050025	4.815636
236.185048	8000.219490	10.597338	-0.050009	4.815608
236.134258	8000.225105	10.602343	-0.050000	4.815610
236.151449	8000.336500	10.607347	-0.050004	4.815642
236.067587	8000.255064	10.612352	-0.049989	4.815619
236.136236	8000.275448	10.617357	-0.050002	4.815624
236.139958	8000.253118	10.622362	-0.050003	4.815618
236.119466	8000.195147	10.627367	-0.050000	4.815601
236.223459	8000.215041	10.632371	-0.050019	4.815606
236.157340	8000.221474	10.637376	-0.050007	4.815608
236.221977	8000.287718	10.642381	-0.050020	4.815627
236.074910	8000.262923	10.647386	-0.049993	4.815621
236.052151	8000.239092	10.652391	-0.049989	4.815614
236.140253	8000.255522	10.657395	-0.050006	4.815618
236.019393	8000.168143	10.662400	-0.049984	4.815593
236.198024	8000.225569	10.667405	-0.050018	4.815609
236.059243	8000.168869	10.672410	-0.049992	4.815593
236.144137	8000.195927	10.677415	-0.050008	4.815601
236.397553	8000.309046	10.682419	-0.050056	4.815633
236.141555	8000.238681	10.687424	-0.050009	4.815613
236.063071	8000.170150	10.692429	-0.049995	4.815594
236.271278	8000.160774	10.697434	-0.050034	4.815590
236.326028	8000.192679	10.702439	-0.050044	4.815599
236.357077	8000.259442	10.707443	-0.050051	4.815618
236.490297	8000.199711	10.712448	-0.050076	4.815600
236.440511	8000.270494	10.717453	-0.050067	4.815621
236.113655	8000.295094	10.722458	-0.050007	4.815630
236.341408	8000.232636	10.727463	-0.050049	4.815611
236.496207	8000.257633	10.732467	-0.050079	4.815617
236.342699	8000.194283	10.737472	-0.050051	4.815599
236.350564	8000.230763	10.742477	-0.050052	4.815610
236.443056	8000.250469	10.747482	-0.050070	4.815615
236.411652	8000.278830	10.752487	-0.050065	4.815624
236.450590	8000.262415	10.757491	-0.050072	4.815619
236.265799	8000.214575	10.762496	-0.050038	4.815606
236.501614	8000.274005	10.767501	-0.050083	4.815622
236.469794	8000.241481	10.772506	-0.050077	4.815612
236.421074	8000.209750	10.777511	-0.050069	4.815603
236.381043	8000.284964	10.782515	-0.050062	4.815626
236.375271	8000.220825	10.787520	-0.050061	4.815607
236.404662	8000.207458	10.792525	-0.050067	4.815603
236.535704	8000.201093	10.797530	-0.050092	4.815600
236.404168	8000.192573	10.802535	-0.050068	4.815598
236.239033	8000.255062	10.807539	-0.050037	4.815617
236.258974	8000.194547	10.812544	-0.050041	4.815600
236.411617	8000.236597	10.817549	-0.050070	4.815611
236.426896	8000.265722	10.822554	-0.050074	4.815620
236.340025	8000.228026	10.827559	-0.050058	4.815609
236.476898	8000.269819	10.832563	-0.050084	4.815621
236.447725	8000.244814	10.837568	-0.050079	4.815613
236.351700	8000.247555	10.842573	-0.050061	4.815615
236.468353	8000.198233	10.847578	-0.050083	4.815600
236.475716	8000.198391	10.852583	-0.050085	4.815600
236.288897	8000.221008	10.857587	-0.050051	4.815607
236.166313	8000.207294	10.862592	-0.050028	4.815604
236.386776	8000.199186	10.867597	-0.050070	4.815600
236.283911	8000.255217	10.872602	-0.050051	4.815617
236.326947	8000.213236	10.877607	-0.050060	4.815605
236.619698	8000.203106	10.882611	-0.050115	4.815600
236.525893	8000.163161	10.887616	-0.050097	4.815589
236.324535	8000.252827	10.892621	-0.050060	4.815616
236.349469	8000.180646	10.897626	-0.050066	4.815595
236.184932	8000.176926	10.902631	-0.050035	4.815595
236.253839	8000.183430	10.907635	-0.050049	4.815596
236.195841	8000.160092	10.912640	-0.050038	4.815590
236.305608	8000.229209	10.917645	-0.050059	4.815609
236.182317	8000.260341	10.922650	-0.050037	4.815619
236.357343	8000.209837	10.927655	-0.050070	4.815603
236.385096	8000.290432	10.932659	-0.050075	4.815627
236.118054	8000.209206	10.937664	-0.050026	4.815604
236.361672	8000.232450	10.942669	-0.050072	4.815610
236.298438	8000.193005	10.947674	-0.050060	4.815599
236.536607	8000.193731	10.952679	-0.050105	4.815598
236.387287	8000.281044	10.957683	-0.050078	4.815624
236.278703	8000.294259	10.962688	-0.050058	4.815628
236.502744	8000.274462	10.967693	-0.050100	4.815621
236.312516	8000.275662	10.972698	-0.050065	4.815623
236.180509	8000.289563	10.977703	-0.050041	4.815627
236.386272	8000.282283	10.982707	-0.050080	4.815624
236.320721	8000.246004	10.987712	-0.050068	4.815614
236.248177	8000.291850	10.992717	-0.050055	4.815628
236.238123	8000.268226	10.997722	-0.050053	4.815621
236.446214	8000.194766	11.002727	-0.050093	4.815598
236.432691	8000.226624	11.007731	-0.050090	4.815608
236.395403	8000.184398	11.012736	-0.050084	4.815596
236.630844	8000.223530	11.017741	-0.050128	4.815606
236.542839	8000.210381	11.022746	-0.050112	4.815602
236.473135	8000.200734	11.027751	-0.050100	4.815600
236.559722	8000.335694	11.032755	-0.050116	4.815639
236.466564	8000.200702	11.037760	-0.050099	4.815600
236.389528	8000.234726	11.042765	-0.050085	4.815610
236.313099	8000.267692	11.047770	-0.050072	4.815620
236.404554	8000.246796	11.052775	-0.050089	4.815614
236.231118	8000.240794	11.057779	-0.050057	4.815613
236.150460	8000.187180	11.062784	-0.050043	4.815597
236.328241	8000.217892	11.067789	-0.050076	4.815606
236.312694	8000.221948	11.072794	-0.050074	4.815607
236.321472	8000.214653	11.077799	-0.050076	4.815605
236.354021	8000.234447	11.082803	-0.050082	4.815610
236.280811	8000.223676	11.087808	-0.050069	4.815607
236.458891	8000.266142	11.092813	-0.050103	4.815619
236.560503	8000.187737	11.097818	-0.050122	4.815596
236.505039	8000.174052	11.102823	-0.050112	4.815592
236.529303	8000.218276	11.107827	-0.050117	4.815605
236.359029	8000.206986	11.112832	-0.050086	4.815602
236.304650	8000.227495	11.117837	-0.050076	4.815608
236.345714	8000.247429	11.122842	-0.050084	4.815614
236.327909	8000.207658	11.127847	-0.050081	4.815602
236.584873	8000.250346	11.132851	-0.050130	4.815614
236.476232	8000.219770	11.137856	-0.050110	4.815605
236.601347	8000.305161	11.142861	-0.050133	4.815630
236.407803	8000.258245	11.147866	-0.050098	4.815617
236.475288	8000.229480	11.152871	-0.050111	4.815608
236.625439	8000.235176	11.157875	-0.050139	4.815609
236.215733	8000.210360	11.162880	-0.050063	4.815604
236.322761	8000.216419	11.167885	-0.050084	4.815605
236.285548	8000.205168	11.172890	-0.050077	4.815602
236.242864	8000.192760	11.177895	-0.050070	4.815598
236.357234	8000.189327	11.182899	-0.050091	4.815597
236.418102	8000.119869	11.187904	-0.050103	4.815576
236.658146	8000.168688	11.192909	-0.050148	4.815589
236.585145	8000.202777	11.197914	-0.050135	4.815600
236.459597	8000.212511	11.202919	-0.050112	4.815603
236.396038	8000.258504	11.207923	-0.050101	4.815617
236.387552	8000.221021	11.212928	-0.050100	4.815606
236.507468	8000.242244	11.217933	-0.050122	4.815611
236.491741	8000.230276	11.222938	-0.050120	4.815608
236.452915	8000.163460	11.227943	-0.050113	4.815589
236.518971	8000.251089	11.232947	-0.050126	4.815614
236.187077	8000.210457	11.237952	-0.050064	4.815604
236.429052	8000.209109	11.242957	-0.050110	4.815602
236.452627	8000.188171	11.247962	-0.050115	4.815596
236.430979	8000.153678	11.252967	-0.050111	4.815586
236.539777	8000.185399	11.257971	-0.050132	4.815595
236.383268	8000.186082	11.262976	-0.050103	4.815596
236.395373	8000.238652	11.267981	-0.050106	4.815611
236.512658	8000.263036	11.272986	-0.050128	4.815617
236.384097	8000.183005	11.277991	-0.050105	4.815595
236.388665	8000.188457	11.282995	-0.050106	4.815596
236.326685	8000.202435	11.288000	-0.050095	4.815601
236.723831	8000.238870	11.293005	-0.050169	4.815609
236.351269	8000.275539	11.298010	-0.050100	4.815622
236.359927	8000.190274	11.303015	-0.050102	4.815597
236.405762	8000.209218	11.308019	-0.050111	4.815602
236.209112	8000.159048	11.313024	-0.050075	4.815588
236.258263	8000.173773	11.318029	-0.050085	4.815592
236.315296	8000.174743	11.323034	-0.050096	4.815592
236.310702	8000.185386	11.328039	-0.050095	4.815596
236.467885	8000.225374	11.333043	-0.050125	4.815606
236.472284	8000.159265	11.338048	-0.050126	4.815587
236.655679	8000.240268	11.343053	-0.050161	4.815610
236.488272	8000.248250	11.348058	-0.050130	4.815613
236.446220	8000.182449	11.353063	-0.050123	4.815594
236.607153	8000.199002	11.358067	-0.050153	4.815598
236.690880	8000.200408	11.363072	-0.050169	4.815598
236.678499	8000.235489	11.368077	-0.050167	4.815608
236.766118	8000.217734	11.373082	-0.050184	4.815603
236.330235	8000.202102	11.378087	-0.050103	4.815600
236.296873	8000.205867	11.383091	-0.050097	4.815601
236.484691	8000.175865	11.388096	-0.050133	4.815592
236.765782	8000.196518	11.393101	-0.050185	4.815596
236.666168	8000.169294	11.398106	-0.050167	4.815589
236.394363	8000.199066	11.403111	-0.050117	4.815599
236.582908	8000.238500	11.408115	-0.050153	4.815610
236.660145	8000.177853	11.413120	-0.050168	4.815592
236.487031	8000.214579	11.418125	-0.050136	4.815603
236.463774	8000.183263	11.423130	-0.050132	4.815594
236.530039	8000.181180	11.428135	-0.050145	4.815593
236.551174	8000.176223	11.433139	-0.050149	4.815592
236.539298	8000.209176	11.438144	-0.050147	4.815601
236.709351	8000.179952	11.443149	-0.050179	4.815592
236.472350	8000.220973	11.448154	-0.050136	4.815605
236.338778	8000.165425	11.453159	-0.050111	4.815589
236.569989	8000.177786	11.458163	-0.050155	4.815592
236.579943	8000.194007	11.463168	-0.050157	4.815596
236.545630	8000.192416	11.468173	-0.050151	4.815596
236.516026	8000.207991	11.473178	-0.050146	4.815601
236.339312	8000.188051	11.478183	-0.050113	4.815596
236.505218	8000.198277	11.483187	-0.050145	4.815598
236.418265	8000.154171	11.488192	-0.050129	4.815586
236.354942	8000.185215	11.493197	-0.050118	4.815595
236.269127	8000.227640	11.498202	-0.050102	4.815608
236.429353	8000.176894	11.503207	-0.050132	4.815592
236.646485	8000.252041	11.508211	-0.050173	4.815613
236.427702	8000.185487	11.513216	-0.050133	4.815595
236.483186	8000.180023	11.518221	-0.050144	4.815593
236.547722	8000.222770	11.523226	-0.050156	4.815605
236.515329	8000.196645	11.528231	-0.050150	4.815597
236.581329	8000.330200	11.533235	-0.050163	4.815636
236.397100	8000.316545	11.538240	-0.050129	4.815633
236.472477	8000.255868	11.543245	-0.050144	4.815615
236.566380	8000.239284	11.548250	-0.050162	4.815610
236.505572	8000.255416	11.553255	-0.050151	4.815615
236.658900	8000.311364	11.558259	-0.050180	4.815630
236.689137	8000.236064	11.563264	-0.050186	4.815608
236.478344	8000.221975	11.568269	-0.050147	4.815605
236.452804	8000.318788	11.573274	-0.050143	4.815633
236.688162	8000.209459	11.578279	-0.050187	4.815600
236.840368	8000.219462	11.583283	-0.050216	4.815602
236.676527	8000.278768	11.588288	-0.050186	4.815621
236.929752	8000.237019	11.593293	-0.050233	4.815607
236.867428	8000.296918	11.598298	-0.050222	4.815625
236.572805	8000.184265	11.603303	-0.050168	4.815593
236.659444	8000.266891	11.608307	-0.050184	4.815617
236.712921	8000.220808	11.613312	-0.050195	4.815603
236.674731	8000.226630	11.618317	-0.050188	4.815605
236.652466	8000.256209	11.623322	-0.050184	4.815614
236.451965	8000.198498	11.628327	-0.050147	4.815598
236.583037	8000.243401	11.633331	-0.050172	4.815611
236.635077	8000.158845	11.638336	-0.050182	4.815586
236.678285	8000.224740	11.643341	-0.050191	4.815605
236.528034	8000.226594	11.648346	-0.050163	4.815606
236.562503	8000.162044	11.653351	-0.050170	4.815587
236.696992	8000.181369	11.658355	-0.050195	4.815592
236.578562	8000.185879	11.663360	-0.050174	4.815594
236.679204	8000.197174	11.668365	-0.050193	4.815596
236.575247	8000.288433	11.673370	-0.050174	4.815624
236.591700	8000.243881	11.678375	-0.050178	4.815611
236.515982	8000.298220	11.683379	-0.050164	4.815627
236.542649	8000.277332	11.688384	-0.050169	4.815621
236.826804	8000.245702	11.693389	-0.050223	4.815610
236.653559	8000.259996	11.698394	-0.050191	4.815615
236.517951	8000.224707	11.703399	-0.050166	4.815605
236.768948	8000.257686	11.708403	-0.050213	4.815614
236.850396	8000.206720	11.713408	-0.050229	4.815598
236.754360	8000.175282	11.718413	-0.050211	4.815590
236.621837	8000.269278	11.723418	-0.050187	4.815618
236.694976	8000.166910	11.728423	-0.050201	4.815587
236.782472	8000.214305	11.733427	-0.050218	4.815601
236.525561	8000.187713	11.738432	-0.050170	4.815594
236.602148	8000.178322	11.743437	-0.050185	4.815591
236.662863	8000.264797	11.748442	-0.050197	4.815616
236.482122	8000.175367	11.753447	-0.050164	4.815591
236.606955	8000.198807	11.758451	-0.050187	4.815597
236.783139	8000.214542	11.763456	-0.050220	4.815601
236.912298	8000.222031	11.768461	-0.050245	4.815602
236.568643	8000.248492	11.773466	-0.050181	4.815612
236.611211	8000.168053	11.778471	-0.050190	4.815588
236.800777	8000.200028	11.783475	-0.050225	4.815596
236.683185	8000.174646	11.788480	-0.050204	4.815590
236.812416	8000.191749	11.793485	-0.050228	4.815594
237.139141	8000.250532	11.798490	-0.050290	4.815610
236.902537	8000.178345	11.803495	-0.050246	4.815590
236.939383	8000.243069	11.808499	-0.050253	4.815608
236.832135	8000.226400	11.813504	-0.050234	4.815604
236.778531	8000.175362	11.818509	-0.050224	4.815589
236.808203	8000.208995	11.823514	-0.050230	4.815599
236.963612	8000.187008	11.828519	-0.050260	4.815592
236.973935	8000.217120	11.833523	-0.050262	4.815601
236.748098	8000.182492	11.838528	-0.050220	4.815592
236.583195	8000.223624	11.843533	-0.050190	4.815604
236.734959	8000.225075	11.848538	-0.050219	4.815604
236.625301	8000.185937	11.853543	-0.050199	4.815593
236.808029	8000.232753	11.858547	-0.050233	4.815606
236.887831	8000.218075	11.863552	-0.050249	4.815601
236.793617	8000.204823	11.868557	-0.050231	4.815598
236.719527	8000.235691	11.873562	-0.050218	4.815607
236.544508	8000.202962	11.878567	-0.050186	4.815598
236.820486	8000.224601	11.883571	-0.050238	4.815603
236.868840	8000.197659	11.888576	-0.050247	4.815595
236.704008	8000.225976	11.893581	-0.050217	4.815604
236.764053	8000.279330	11.898586	-0.050229	4.815620
236.666090	8000.222227	11.903591	-0.050211	4.815603
236.792709	8000.237151	11.908595	-0.050235	4.815607
236.613098	8000.184054	11.913600	-0.050202	4.815592
236.676938	8000.216109	11.918605	-0.050214	4.815601
236.787599	8000.216888	11.923610	-0.050235	4.815601
236.730158	8000.168992	11.928615	-0.050225	4.815587
236.837066	8000.269039	11.933619	-0.050245	4.815616
236.637063	8000.181430	11.938624	-0.050208	4.815592
236.564035	8000.185614	11.943629	-0.050195	4.815593
236.785393	8000.236265	11.948634	-0.050237	4.815607
236.659950	8000.216095	11.953639	-0.050214	4.815601
236.745885	8000.260260	11.958643	-0.050230	4.815614
236.745898	8000.189806	11.963648	-0.050231	4.815593
236.808772	8000.205824	11.968653	-0.050243	4.815598
236.743597	8000.219749	11.973658	-0.050231	4.815602
236.680251	8000.167484	11.978663	-0.050220	4.815587
237.020348	8000.200852	11.983667	-0.050284	4.815595
236.773197	8000.192576	11.988672	-0.050238	4.815594
236.783124	8000.201321	11.993677	-0.050240	4.815596
236.930528	8000.175999	11.998682	-0.050268	4.815588
236.825631	8000.213840	12.003687	-0.050249	4.815600
236.925993	8000.282807	12.008691	-0.050268	4.815620
236.739919	8000.257372	12.013696	-0.050234	4.815613
236.925417	8000.216652	12.018701	-0.050269	4.815600
236.879563	8000.204192	12.023706	-0.050261	4.815597
236.687186	8000.175451	12.028711	-0.050225	4.815589
236.922504	8000.242351	12.033715	-0.050270	4.815608
236.777798	8000.246431	12.038720	-0.050243	4.815610
236.787137	8000.213512	12.043725	-0.050245	4.815600
236.946247	8000.219355	12.048730	-0.050275	4.815601
236.944247	8000.185182	12.053735	-0.050275	4.815591
236.722268	8000.178386	12.058739	-0.050234	4.815590
236.872165	8000.181943	12.063744	-0.050263	4.815590
236.974791	8000.180454	12.068749	-0.050282	4.815589
236.882389	8000.166164	12.073754	-0.050266	4.815586
236.978425	8000.183793	12.078759	-0.050284	4.815590
236.858884	8000.221395	12.083763	-0.050262	4.815602
236.788708	8000.211740	12.088768	-0.050249	4.815599
236.707125	8000.190151	12.093773	-0.050235	4.815593
237.006119	8000.237800	12.098778	-0.050291	4.815606
236.998255	8000.165080	12.103783	-0.050290	4.815585
236.953827	8000.239156	12.108787	-0.050282	4.815606
236.841119	8000.210649	12.113792	-0.050261	4.815599
236.831031	8000.196637	12.118797	-0.050260	4.815595
236.927389	8000.249518	12.123802	-0.050278	4.815610
236.827005	8000.180626	12.128807	-0.050260	4.815590
237.036338	8000.208652	12.133811	-0.050299	4.815597
237.099119	8000.191559	12.138816	-0.050311	4.815592
236.824952	8000.207407	12.143821	-0.050261	4.815598
236.978861	8000.262297	12.148826	-0.050290	4.815613
236.884726	8000.226617	12.153831	-0.050273	4.815603
236.756734	8000.268352	12.158835	-0.050249	4.815616
236.848698	8000.229307	12.163840	-0.050267	4.815604
236.885121	8000.190422	12.168845	-0.050274	4.815592
236.916500	8000.193109	12.173850	-0.050280	4.815593
236.808739	8000.173227	12.178855	-0.050261	4.815588
237.044703	8000.197417	12.183859	-0.050305	4.815594
237.184851	8000.194406	12.188864	-0.050332	4.815592
236.977606	8000.214552	12.193869	-0.050294	4.815599
236.949371	8000.198107	12.198874	-0.050289	4.815594
236.948108	8000.162878	12.203879	-0.050289	4.815584
237.120976	8000.220214	12.208883	-0.050322	4.815600
236.908095	8000.218906	12.213888	-0.050282	4.815601
236.631054	8000.202665	12.218893	-0.050231	4.815597
236.734152	8000.216137	12.223898	-0.050251	4.815601
236.654725	8000.162541	12.228903	-0.050236	4.815585
236.542200	8000.208802	12.233907	-0.050216	4.815599
236.752353	8000.204799	12.238912	-0.050255	4.815597
236.793802	8000.182017	12.243917	-0.050264	4.815590
236.737691	8000.211043	12.248922	-0.050254	4.815599
236.617951	8000.185626	12.253927	-0.050232	4.815592
236.713362	8000.224605	12.258931	-0.050250	4.815603
236.794061	8000.215282	12.263936	-0.050265	4.815600
236.741871	8000.186697	12.268941	-0.050256	4.815592
236.861690	8000.198306	12.273946	-0.050279	4.815595
236.588141	8000.165034	12.278951	-0.050228	4.815586
236.791883	8000.211125	12.283955	-0.050267	4.815599
236.827895	8000.207479	12.288960	-0.050274	4.815597
236.674668	8000.191127	12.293965	-0.050246	4.815593
236.864226	8000.172902	12.298970	-0.050281	4.815587
236.716399	8000.155570	12.303975	-0.050254	4.815583
236.951065	8000.184010	12.308979	-0.050298	4.815590
236.634467	8000.189552	12.313984	-0.050240	4.815593
236.637126	8000.171476	12.318989	-0.050241	4.815588
236.935634	8000.193483	12.323994	-0.050297	4.815593
236.842300	8000.138592	12.328999	-0.050280	4.815577
236.806547	8000.196788	12.334003	-0.050274	4.815594
236.684255	8000.159580	12.339008	-0.050251	4.815584
236.885841	8000.170391	12.344013	-0.050289	4.815586
236.891536	8000.205767	12.349018	-0.050291	4.815596
236.805436	8000.172355	12.354023	-0.050275	4.815587
236.656127	8000.174224	12.359027	-0.050248	4.815588
236.785276	8000.155012	12.364032	-0.050272	4.815582
236.920506	8000.149784	12.369037	-0.050298	4.815580
236.974421	8000.173133	12.374042	-0.050308	4.815587
236.728315	8000.128560	12.379047	-0.050263	4.815575
236.661171	8000.188380	12.384051	-0.050251	4.815592
236.956983	8000.171893	12.389056	-0.050306	4.815586
236.938247	8000.173760	12.394061	-0.050303	4.815587
236.965273	8000.192397	12.399066	-0.050309	4.815592
236.867396	8000.178017	12.404071	-0.050291	4.815588
237.153554	8000.203028	12.409075	-0.050345	4.815594
237.005053	8000.176071	12.414080	-0.050318	4.815587
236.956262	8000.164630	12.419085	-0.050309	4.815584
237.182795	8000.181189	12.424090	-0.050351	4.815588
237.084357	8000.147575	12.429095	-0.050334	4.815578
237.153122	8000.187188	12.434099	-0.050347	4.815590
237.162315	8000.166015	12.439104	-0.050349	4.815583
237.104314	8000.181125	12.444109	-0.050339	4.815588
237.091034	8000.203375	12.449114	-0.050337	4.815595
236.913724	8000.188764	12.454119	-0.050304	4.815591
237.210159	8000.226760	12.459123	-0.050360	4.815601
236.908366	8000.283810	12.464128	-0.050304	4.815619
237.011553	8000.189409	12.469133	-0.050323	4.815591
237.172733	8000.255099	12.474138	-0.050354	4.815609
237.015805	8000.255774	12.479143	-0.050325	4.815610
237.054339	8000.242557	12.484147	-0.050333	4.815606
237.075275	8000.226916	12.489152	-0.050337	4.815601
237.030320	8000.249716	12.494157	-0.050329	4.815608
236.967064	8000.246583	12.499162	-0.050318	4.815608
237.001874	8000.249326	12.504167	-0.050325	4.815608
237.156860	8000.220925	12.509171	-0.050354	4.815599
236.928175	8000.214018	12.514176	-0.050312	4.815598
237.029925	8000.193290	12.519181	-0.050331	4.815592
236.927618	8000.269624	12.524186	-0.050313	4.815615
236.936538	8000.199315	12.529191	-0.050315	4.815594
236.890227	8000.227433	12.534195	-0.050306	4.815602
236.964999	8000.235102	12.539200	-0.050321	4.815604
236.807404	8000.186635	12.544205	-0.050292	4.815591
236.817604	8000.207133	12.549210	-0.050294	4.815597
236.955866	8000.174186	12.554215	-0.050320	4.815587
237.141390	8000.200755	12.559219	-0.050355	4.815593
236.915848	8000.178947	12.564224	-0.050314	4.815588
236.828454	8000.186100	12.569229	-0.050298	4.815591
237.000169	8000.206035	12.574234	-0.050330	4.815596
236.954659	8000.170082	12.579239	-0.050322	4.815585
236.956072	8000.186164	12.584243	-0.050323	4.815590
237.012790	8000.164699	12.589248	-0.050334	4.815583
237.026905	8000.226916	12.594253	-0.050337	4.815601
237.096257	8000.188569	12.599258	-0.050350	4.815590
237.077334	8000.161596	12.604263	-0.050347	4.815582
237.082830	8000.193765	12.609267	-0.050349	4.815592
237.094497	8000.169428	12.614272	-0.050351	4.815584
237.007514	8000.163771	12.619277	-0.050336	4.815583
237.264058	8000.184025	12.624282	-0.050384	4.815588
237.316281	8000.166760	12.629287	-0.050394	4.815582
237.106563	8000.212499	12.634291	-0.050355	4.815597
237.024992	8000.217611	12.639296	-0.050341	4.815599
236.950643	8000.202548	12.644301	-0.050327	4.815595
236.912622	8000.212645	12.649306	-0.050320	4.815598
236.737296	8000.170297	12.654311	-0.050288	4.815586
236.808921	8000.216364	12.659315	-0.050302	4.815599
236.779148	8000.190282	12.664320	-0.050297	4.815592
236.772447	8000.219048	12.669325	-0.050296	4.815600
236.835314	8000.199820	12.674330	-0.050308	4.815594
236.918397	8000.160630	12.679335	-0.050324	4.815582
236.956647	8000.206152	12.684339	-0.050332	4.815596
237.025648	8000.260722	12.689344	-0.050345	4.815611
236.979786	8000.183108	12.694349	-0.050337	4.815589
237.101353	8000.286601	12.699354	-0.050360	4.815618
236.962115	8000.218141	12.704359	-0.050334	4.815599
237.030816	8000.231051	12.709363	-0.050348	4.815602
237.061360	8000.247609	12.714368	-0.050354	4.815607
236.833004	8000.206530	12.719373	-0.050312	4.815596
236.903573	8000.247240	12.724378	-0.050325	4.815608
237.106394	8000.219621	12.729383	-0.050363	4.815599
237.028034	8000.227989	12.734387	-0.050349	4.815601
236.894189	8000.175639	12.739392	-0.050325	4.815587
237.018820	8000.174510	12.744397	-0.050348	4.815586
237.122064	8000.198666	12.749402	-0.050368	4.815592
237.072775	8000.194693	12.754407	-0.050359	4.815592
237.138916	8000.197949	12.759411	-0.050372	4.815592
236.995113	8000.198839	12.764416	-0.050346	4.815593
237.001593	8000.204323	12.769421	-0.050347	4.815595
237.052364	8000.220144	12.774426	-0.050357	4.815599
237.085861	8000.201504	12.779431	-0.050364	4.815593
237.158757	8000.213415	12.784435	-0.050378	4.815596
237.110913	8000.268210	12.789440	-0.050369	4.815613
237.024162	8000.203812	12.794445	-0.050354	4.815594
236.895339	8000.243398	12.799450	-0.050330	4.815606
236.915498	8000.195702	12.804455	-0.050334	4.815592
237.139157	8000.202602	12.809459	-0.050376	4.815593
237.112767	8000.205412	12.814464	-0.050372	4.815594
236.997252	8000.177927	12.819469	-0.050351	4.815587
236.894331	8000.227549	12.824474	-0.050332	4.815602
236.958324	8000.215816	12.829479	-0.050344	4.815598
237.215995	8000.228613	12.834483	-0.050393	4.815601
237.266616	8000.234819	12.839488	-0.050403	4.815602
236.916063	8000.188536	12.844493	-0.050338	4.815590
237.100820	8000.202276	12.849498	-0.050373	4.815593
236.880713	8000.222212	12.854503	-0.050332	4.815600
237.022751	8000.240594	12.859507	-0.050359	4.815605
236.997488	8000.235946	12.864512	-0.050355	4.815604
236.807966	8000.199774	12.869517	-0.050320	4.815594
236.864471	8000.254139	12.874522	-0.050331	4.815610
237.035247	8000.235608	12.879527	-0.050363	4.815603
236.989116	8000.212462	12.884531	-0.050355	4.815597
236.839343	8000.242092	12.889536	-0.050327	4.815606
236.923205	8000.242433	12.894541	-0.050343	4.815606
237.004114	8000.285450	12.899546	-0.050359	4.815618
236.796323	8000.244706	12.904551	-0.050321	4.815607
236.976941	8000.228472	12.909555	-0.050355	4.815601
236.967646	8000.182431	12.914560	-0.050353	4.815588
236.896442	8000.189848	12.919565	-0.050341	4.815591
236.859521	8000.207439	12.924570	-0.050334	4.815596
237.127936	8000.167008	12.929575	-0.050385	4.815583
237.101045	8000.230690	12.934579	-0.050380	4.815601
236.918305	8000.195697	12.939584	-0.050346	4.815592
237.005067	8000.160839	12.944589	-0.050363	4.815582
237.092133	8000.226385	12.949594	-0.050380	4.815600
236.969297	8000.142172	12.954599	-0.050357	4.815576
237.010099	8000.184532	12.959603	-0.050365	4.815588
236.894857	8000.168800	12.964608	-0.050344	4.815584
236.967548	8000.172163	12.969613	-0.050358	4.815585
237.087248	8000.277762	12.974618	-0.050381	4.815615
236.913909	8000.296326	12.979623	-0.050349	4.815621
236.970002	8000.236400	12.984627	-0.050360	4.815604
237.036199	8000.223636	12.989632	-0.050373	4.815600
236.996760	8000.167488	12.994637	-0.050366	4.815583
237.163688	8000.230069	12.999642	-0.050397	4.815601
237.073861	8000.191254	13.004647	-0.050381	4.815590
237.070750	8000.242509	13.009651	-0.050381	4.815605
237.099621	8000.228066	13.014656	-0.050387	4.815601
236.933284	8000.199749	13.019661	-0.050356	4.815593
237.042751	8000.197305	13.024666	-0.050377	4.815592
237.186529	8000.190081	13.029671	-0.050404	4.815589
237.283497	8000.218407	13.034675	-0.050423	4.815597
237.038199	8000.242202	13.039680	-0.050377	4.815605
237.040906	8000.165383	13.044685	-0.050378	4.815582
236.873144	8000.200059	13.049690	-0.050347	4.815593
236.858184	8000.171014	13.054695	-0.050345	4.815585
237.029595	8000.217647	13.059699	-0.050377	4.815598
237.040274	8000.191157	13.064704	-0.050380	4.815590
236.884364	8000.163011	13.069709	-0.050351	4.815582
236.840917	8000.196516	13.074714	-0.050344	4.815592
236.861977	8000.190490	13.079719	-0.050348	4.815591
237.037079	8000.200868	13.084723	-0.050381	4.815593
237.190216	8000.229044	13.089728	-0.050410	4.815600
237.011994	8000.175967	13.094733	-0.050377	4.815586
237.089752	8000.236021	13.099738	-0.050392	4.815603
237.069178	8000.231450	13.104743	-0.050389	4.815601
236.969374	8000.206358	13.109747	-0.050371	4.815595
237.165347	8000.234166	13.114752	-0.050407	4.815602
237.145035	8000.192217	13.119757	-0.050404	4.815590
237.195275	8000.225119	13.124762	-0.050414	4.815599
237.003254	8000.214539	13.129767	-0.050379	4.815597
237.077445	8000.223267	13.134771	-0.050393	4.815599
237.180408	8000.200422	13.139776	-0.050412	4.815592
237.146882	8000.213797	13.144781	-0.050407	4.815596
237.270238	8000.240418	13.149786	-0.050430	4.815603
237.010932	8000.209512	13.154791	-0.050382	4.815595
236.910102	8000.222854	13.159795	-0.050364	4.815600
237.313562	8000.244444	13.164800	-0.050439	4.815604
237.042239	8000.226159	13.169805	-0.050389	4.815600
237.073285	8000.256611	13.174810	-0.050395	4.815609
237.215352	8000.273925	13.179815	-0.050422	4.815613
237.173361	8000.258323	13.184819	-0.050415	4.815609
237.165620	8000.277460	13.189824	-0.050414	4.815614
237.054865	8000.222281	13.194829	-0.050394	4.815599
237.090042	8000.217554	13.199834	-0.050401	4.815597
237.231076	8000.223103	13.204839	-0.050427	4.815598
237.136949	8000.237622	13.209843	-0.050410	4.815603
237.229071	8000.243439	13.214848	-0.050428	4.815604
237.387862	8000.175580	13.219853	-0.050458	4.815583
237.301191	8000.230809	13.224858	-0.050442	4.815600
237.178135	8000.179702	13.229863	-0.050420	4.815586
237.302444	8000.188181	13.234867	-0.050443	4.815587
237.307042	8000.229950	13.239872	-0.050445	4.815600
237.047733	8000.207588	13.244877	-0.050397	4.815594
237.122347	8000.252638	13.249882	-0.050411	4.815607
237.212504	8000.206086	13.254887	-0.050428	4.815593
237.126951	8000.226086	13.259891	-0.050413	4.815599
237.265343	8000.260430	13.264896	-0.050439	4.815609
237.144866	8000.221114	13.269901	-0.050417	4.815598
237.272581	8000.237126	13.274906	-0.050441	4.815602
237.125035	8000.192027	13.279911	-0.050414	4.815589
237.287393	8000.212878	13.284915	-0.050445	4.815595
237.265458	8000.260621	13.289920	-0.050441	4.815609
237.103331	8000.189649	13.294925	-0.050411	4.815589
237.356185	8000.231206	13.299930	-0.050459	4.815600
237.306731	8000.266749	13.304935	-0.050450	4.815610
237.058559	8000.243502	13.309939	-0.050404	4.815605
237.204291	8000.306805	13.314944	-0.050432	4.815622
237.283167	8000.279294	13.319949	-0.050447	4.815614
237.235139	8000.289227	13.324954	-0.050438	4.815617
237.027075	8000.371308	13.329959	-0.050400	4.815642
237.391258	8000.289720	13.334963	-0.050468	4.815616
237.462788	8000.310154	13.339968	-0.050482	4.815622
237.320549	8000.275822	13.344973	-0.050456	4.815613
237.319211	8000.291859	13.349978	-0.050456	4.815617
237.459953	8000.246135	13.354983	-0.050483	4.815603
237.445551	8000.214962	13.359987	-0.050481	4.815594
237.444067	8000.182933	13.364992	-0.050481	4.815585
237.352417	8000.178267	13.369997	-0.050464	4.815584
237.367296	8000.216999	13.375002	-0.050467	4.815595
237.246171	8000.212919	13.380007	-0.050445	4.815595
237.324995	8000.252698	13.385011	-0.050460	4.815606
237.242002	8000.312259	13.390016	-0.050445	4.815624
237.055011	8000.249425	13.395021	-0.050411	4.815606
237.189395	8000.276227	13.400026	-0.050436	4.815613
237.180060	8000.286793	13.405031	-0.050435	4.815616
237.160714	8000.245926	13.410035	-0.050432	4.815605
237.458615	8000.268995	13.415040	-0.050488	4.815610
237.321207	8000.261444	13.420045	-0.050463	4.815608
237.284301	8000.267287	13.425050	-0.050456	4.815610
237.140075	8000.261761	13.430055	-0.050430	4.815609
237.139205	8000.248967	13.435059	-0.050430	4.815606
237.267227	8000.229737	13.440064	-0.050454	4.815599
237.138071	8000.177462	13.445069	-0.050431	4.815585
237.066339	8000.238276	13.450074	-0.050418	4.815603
237.185907	8000.254154	13.455079	-0.050440	4.815607
237.346289	8000.248271	13.460083	-0.050471	4.815604
237.271383	8000.272718	13.465088	-0.050457	4.815612
237.376367	8000.196502	13.470093	-0.050477	4.815589
237.428287	8000.220887	13.475098	-0.050487	4.815596
237.256056	8000.192473	13.480103	-0.050456	4.815588
237.288093	8000.224009	13.485107	-0.050462	4.815597
237.209520	8000.248396	13.490112	-0.050448	4.815605
237.070024	8000.261105	13.495117	-0.050422	4.815609
237.350145	8000.311653	13.500122	-0.050475	4.815623
237.374525	8000.233051	13.505127	-0.050480	4.815600
237.088304	8000.249768	13.510131	-0.050427	4.815606
237.322464	8000.272862	13.515136	-0.050471	4.815611
237.169477	8000.218060	13.520141	-0.050443	4.815596
237.466630	8000.267819	13.525146	-0.050499	4.815609
237.267951	8000.228291	13.530151	-0.050462	4.815599
237.215148	8000.232806	13.535155	-0.050453	4.815600
237.176883	8000.245034	13.540160	-0.050446	4.815604
237.161085	8000.201022	13.545165	-0.050444	4.815591
237.257820	8000.213323	13.550170	-0.050462	4.815594
237.291074	8000.226722	13.555175	-0.050469	4.815598
237.255310	8000.235787	13.560179	-0.050462	4.815601
237.275116	8000.258579	13.565184	-0.050467	4.815607
237.251040	8000.229384	13.570189	-0.050462	4.815599
237.450740	8000.307456	13.575194	-0.050500	4.815621
237.398027	8000.323721	13.580199	-0.050491	4.815626
237.210332	8000.244853	13.585203	-0.050456	4.815604
237.204077	8000.236243	13.590208	-0.050455	4.815601
237.231574	8000.202552	13.595213	-0.050461	4.815591
237.229129	8000.258090	13.600218	-0.050461	4.815607
237.405944	8000.250340	13.605223	-0.050494	4.815604
237.402503	8000.223619	13.610227	-0.050494	4.815596
237.336470	8000.235393	13.615232	-0.050482	4.815600
237.519030	8000.218124	13.620237	-0.050517	4.815594
237.322942	8000.254473	13.625242	-0.050481	4.815606
237.177016	8000.292711	13.630247	-0.050454	4.815618
237.203870	8000.225898	13.635251	-0.050459	4.815598
237.486756	8000.212406	13.640256	-0.050512	4.815593
237.274590	8000.186543	13.645261	-0.050473	4.815586
237.278230	8000.232568	13.650266	-0.050474	4.815600
237.256133	8000.221563	13.655271	-0.050471	4.815596
237.365776	8000.228735	13.660275	-0.050492	4.815598
237.374723	8000.307959	13.665280	-0.050494	4.815621
237.354025	8000.204052	13.670285	-0.050490	4.815591
237.503461	8000.211875	13.675290	-0.050518	4.815592
237.456264	8000.231434	13.680295	-0.050510	4.815598
237.366441	8000.243888	13.685299	-0.050494	4.815602
237.434779	8000.255725	13.690304	-0.050507	4.815606
237.491782	8000.197949	13.695309	-0.050518	4.815588
237.449266	8000.219722	13.700314	-0.050510	4.815595
237.382826	8000.235762	13.705319	-0.050499	4.815600
237.518171	8000.212380	13.710323	-0.050524	4.815592
237.476113	8000.230955	13.715328	-0.050517	4.815598
237.226777	8000.233322	13.720333	-0.050471	4.815600
237.346105	8000.227835	13.725338	-0.050493	4.815598
237.202987	8000.265051	13.730343	-0.050467	4.815609
237.307574	8000.219803	13.735347	-0.050487	4.815596
237.349674	8000.242960	13.740352	-0.050495	4.815602
237.381299	8000.212540	13.745357	-0.050502	4.815593
237.356602	8000.248489	13.750362	-0.050498	4.815604
237.458490	8000.233104	13.755367	-0.050517	4.815599
237.306094	8000.278713	13.760371	-0.050489	4.815613
237.467069	8000.365765	13.765376	-0.050519	4.815637
237.253210	8000.224518	13.770381	-0.050480	4.815597
237.389956	8000.235338	13.775386	-0.050506	4.815600
237.232691	8000.234939	13.780391	-0.050477	4.815600
237.284798	8000.220876	13.785395	-0.050487	4.815596
237.305069	8000.230858	13.790400	-0.050491	4.815599
237.317286	8000.214006	13.795405	-0.050494	4.815594
237.371075	8000.288623	13.800410	-0.050505	4.815615
237.458338	8000.267658	13.805415	-0.050521	4.815609
237.368107	8000.239517	13.810419	-0.050505	4.815601
237.372880	8000.231088	13.815424	-0.050506	4.815598
237.334878	8000.190984	13.820429	-0.050499	4.815587
237.512150	8000.239850	13.825434	-0.050533	4.815600
237.575560	8000.185384	13.830439	-0.050545	4.815584
237.525908	8000.225197	13.835443	-0.050536	4.815596
237.537286	8000.193378	13.840448	-0.050539	4.815587
237.451655	8000.190947	13.845453	-0.050523	4.815586
237.639559	8000.218625	13.850458	-0.050559	4.815593
237.568759	8000.260229	13.855463	-0.050546	4.815606
237.536624	8000.212744	13.860467	-0.050540	4.815592
237.596138	8000.230845	13.865472	-0.050552	4.815597
237.326402	8000.200835	13.870477	-0.050502	4.815590
237.308756	8000.295645	13.875482	-0.050499	4.815617
237.416082	8000.350844	13.880487	-0.050520	4.815633
237.389097	8000.224404	13.885491	-0.050515	4.815596
237.327953	8000.276846	13.890496	-0.050504	4.815612
237.436873	8000.228465	13.895501	-0.050525	4.815597
237.510945	8000.233987	13.900506	-0.050539	4.815598
237.165549	8000.181378	13.905511	-0.050475	4.815585
237.149036	8000.229210	13.910515	-0.050473	4.815599
237.425182	8000.247651	13.915520	-0.050524	4.815603
237.256383	8000.241722	13.920525	-0.050493	4.815602
237.214658	8000.277393	13.925530	-0.050486	4.815612
237.337145	8000.252732	13.930535	-0.050509	4.815605
237.344145	8000.266769	13.935539	-0.050511	4.815609
237.387061	8000.333732	13.940544	-0.050520	4.815628
237.446051	8000.306964	13.945549	-0.050531	4.815620
237.318725	8000.293169	13.950554	-0.050508	4.815616
237.250795	8000.323070	13.955559	-0.050495	4.815626
237.237852	8000.271627	13.960563	-0.050493	4.815611
237.390982	8000.316895	13.965568	-0.050522	4.815623
237.308568	8000.263247	13.970573	-0.050507	4.815608
237.386315	8000.311553	13.975578	-0.050522	4.815621
237.386639	8000.346844	13.980583	-0.050523	4.815632
237.132913	8000.248737	13.985587	-0.050476	4.815604
237.321978	8000.259344	13.990592	-0.050512	4.815606
237.274305	8000.220151	13.995597	-0.050503	4.815595
237.332161	8000.247837	14.000602	-0.050514	4.815603
237.272161	8000.265051	14.005607	-0.050504	4.815608
237.232104	8000.220641	14.010611	-0.050497	4.815596
237.502214	8000.227235	14.015616	-0.050547	4.815596
237.343426	8000.197972	14.020621	-0.050518	4.815588
237.254984	8000.249967	14.025626	-0.050502	4.815604
237.317941	8000.294827	14.030631	-0.050514	4.815617
237.371552	8000.270108	14.035635	-0.050525	4.815609
237.286183	8000.320018	14.040640	-0.050509	4.815624
237.466086	8000.238619	14.045645	-0.050543	4.815600
237.540595	8000.246284	14.050650	-0.050558	4.815601
237.331854	8000.312333	14.055655	-0.050519	4.815622
237.393736	8000.215118	14.060659	-0.050531	4.815593
237.564193	8000.317279	14.065664	-0.050563	4.815622
237.379118	8000.223499	14.070669	-0.050529	4.815596
237.441255	8000.240575	14.075674	-0.050541	4.815600
237.464805	8000.249543	14.080679	-0.050546	4.815603
237.544303	8000.261562	14.085683	-0.050561	4.815606
237.597522	8000.296650	14.090688	-0.050572	4.815616
237.446907	8000.267521	14.095693	-0.050544	4.815608
237.453308	8000.287957	14.100698	-0.050546	4.815614
237.406227	8000.326744	14.105703	-0.050537	4.815626
237.328372	8000.265694	14.110707	-0.050523	4.815608
237.417380	8000.315253	14.115712	-0.050540	4.815622
237.231597	8000.236415	14.120717	-0.050506	4.815600
237.209560	8000.245706	14.125722	-0.050502	4.815603
237.320053	8000.294548	14.130727	-0.050523	4.815616
237.554068	8000.247145	14.135731	-0.050567	4.815601
237.523386	8000.323585	14.140736	-0.050562	4.815624
237.494773	8000.243046	14.145741	-0.050557	4.815601
237.608043	8000.276981	14.150746	-0.050579	4.815610
237.522606	8000.331162	14.155751	-0.050563	4.815626
237.386803	8000.246733	14.160755	-0.050538	4.815602
237.570602	8000.257255	14.165760	-0.050573	4.815604
237.423049	8000.266627	14.170765	-0.050546	4.815608
237.598817	8000.326151	14.175770	-0.050579	4.815624
237.524958	8000.320708	14.180775	-0.050566	4.815623
237.427811	8000.299930	14.185779	-0.050548	4.815617
237.748874	8000.359696	14.190784	-0.050608	4.815633
237.479004	8000.270936	14.195789	-0.050559	4.815609
237.452128	8000.300441	14.200794	-0.050554	4.815617
237.370628	8000.337597	14.205799	-0.050539	4.815629
237.298888	8000.303349	14.210803	-0.050526	4.815619
237.570929	8000.349495	14.215808	-0.050577	4.815631
237.513058	7999.294391	14.220813	-0.050566	4.815323

237.152480	7996.071927	14.225818	-0.050498	4.814383
237.249335	7990.608229	14.230823	-0.050512	4.812785
237.481527	7983.933079	14.235827	-0.050552	4.810831
237.407231	7976.612576	14.240832	-0.050534	4.808689
237.304993	7968.981504	14.245837	-0.050510	4.806455
237.645357	7961.213800	14.250842	-0.050569	4.804178
237.541149	7953.382180	14.255847	-0.050545	4.801883
237.424770	7945.345518	14.260851	-0.050518	4.799528
237.453615	7937.471420	14.265856	-0.050519	4.797218
237.271748	7929.372563	14.270861	-0.050480	4.794841
237.178758	7921.382190	14.275866	-0.050458	4.792496
237.087046	7913.356480	14.280871	-0.050436	4.790138
237.049005	7905.400296	14.285875	-0.050424	4.787800
236.997665	7897.396890	14.290880	-0.050410	4.785446
236.876511	7889.429380	14.295885	-0.050383	4.783103
237.211623	7881.395637	14.300890	-0.050440	4.780737
237.077691	7873.426286	14.305895	-0.050411	4.778390
236.960116	7865.409217	14.310899	-0.050384	4.776028
236.967227	7857.420010	14.315904	-0.050380	4.773673
236.818190	7849.394668	14.320909	-0.050348	4.771307
236.878653	7841.356957	14.325914	-0.050354	4.768934
236.746530	7833.402260	14.330919	-0.050325	4.766586
236.951387	7825.300298	14.335923	-0.050358	4.764192
236.908677	7817.450744	14.340928	-0.050346	4.761873
236.740249	7809.374493	14.345933	-0.050309	4.759485
236.824225	7801.400239	14.350938	-0.050320	4.757126
236.696999	7793.393772	14.355943	-0.050292	4.754757
236.593181	7785.286211	14.360947	-0.050268	4.752356
236.604409	7777.303100	14.365952	-0.050265	4.749991
236.670215	7769.325611	14.370957	-0.050272	4.747626
236.728804	7761.299380	14.375962	-0.050279	4.745246
236.519580	7753.381676	14.380967	-0.050235	4.742897
236.471122	7745.325580	14.385971	-0.050221	4.740505
236.443678	7737.373617	14.390976	-0.050211	4.738144
236.432826	7729.329170	14.395981	-0.050204	4.735753
236.337362	7721.349920	14.400986	-0.050182	4.733381
236.248744	7713.338056	14.405991	-0.050160	4.730998
236.166522	7705.317744	14.410995	-0.050140	4.728611
236.169423	7697.341072	14.416000	-0.050136	4.726236
236.358302	7689.320821	14.421005	-0.050166	4.723846
236.323193	7681.320428	14.426010	-0.050155	4.721462
236.339969	7673.339190	14.431015	-0.050154	4.719081
236.262332	7665.334002	14.436019	-0.050134	4.716693
236.324976	7657.294307	14.441024	-0.050141	4.714293
236.012228	7649.298581	14.446029	-0.050078	4.711905
235.891527	7641.261508	14.451034	-0.050051	4.709504
235.800208	7633.310236	14.456039	-0.050029	4.707127
235.777162	7625.284221	14.461043	-0.050020	4.704726
235.922555	7617.367803	14.466048	-0.050042	4.702356
235.824485	7609.286870	14.471053	-0.050019	4.699937
235.738863	7601.355040	14.476058	-0.049999	4.697561
235.648553	7593.325187	14.481063	-0.049977	4.695154
235.676949	7585.264858	14.486067	-0.049977	4.692737
235.715690	7577.243070	14.491072	-0.049980	4.690330
235.785617	7569.278601	14.496077	-0.049988	4.687938
235.861922	7561.257943	14.501082	-0.049997	4.685529
235.906687	7553.326380	14.506087	-0.050001	4.683146
235.786852	7545.326337	14.511091	-0.049974	4.680740
235.795379	7537.321783	14.516096	-0.049971	4.678332
235.534449	7529.318981	14.521101	-0.049917	4.675924
235.436232	7521.227905	14.526106	-0.049894	4.673488
235.419258	7513.136286	14.531111	-0.049886	4.671050
235.321052	7505.184184	14.536115	-0.049863	4.668653
235.461768	7497.234108	14.541120	-0.049885	4.666255
235.206135	7489.215121	14.546125	-0.049832	4.663835
235.216647	7481.264474	14.551130	-0.049829	4.661434
235.268972	7473.224052	14.556135	-0.049834	4.659006
235.377602	7465.227244	14.561139	-0.049850	4.656589
235.166053	7457.255200	14.566144	-0.049806	4.654178
235.208052	7449.193232	14.571149	-0.049809	4.651739
235.267061	7441.211833	14.576154	-0.049815	4.649323
235.249087	7433.256006	14.581159	-0.049807	4.646913
235.136022	7425.185637	14.586163	-0.049781	4.644468
235.339916	7417.254113	14.591168	-0.049814	4.642063
235.109698	7409.204322	14.596173	-0.049766	4.639621
234.790161	7401.254337	14.601178	-0.049702	4.637208
234.865238	7393.210608	14.606183	-0.049711	4.634766
235.006309	7385.158868	14.611187	-0.049733	4.632319
234.825823	7377.151993	14.616192	-0.049694	4.629885
235.040469	7369.172411	14.621197	-0.049730	4.627458
234.779064	7361.170873	14.626202	-0.049676	4.625024
234.912260	7353.198537	14.631207	-0.049696	4.622596
234.826777	7345.189250	14.636211	-0.049675	4.620156
235.028524	7337.227335	14.641216	-0.049708	4.617730
234.720615	7329.158934	14.646221	-0.049646	4.615269
234.429589	7321.147134	14.651226	-0.049587	4.612825
234.565837	7313.171280	14.656231	-0.049608	4.610390
234.490118	7305.134294	14.661235	-0.049589	4.607935
234.525000	7297.137300	14.666240	-0.049591	4.605491
234.467977	7289.185455	14.671245	-0.049575	4.603060
234.625385	7281.196808	14.676250	-0.049600	4.600616
234.499538	7273.200466	14.681255	-0.049572	4.598168
234.292973	7265.144348	14.686259	-0.049528	4.595701
234.409648	7257.131844	14.691264	-0.049545	4.593246
234.304355	7249.086322	14.696269	-0.049521	4.590779
234.187120	7241.136772	14.701274	-0.049494	4.588340
234.210371	7233.094581	14.706279	-0.049494	4.585872
234.260047	7225.152197	14.711283	-0.049498	4.583433
234.283635	7217.163302	14.716288	-0.049498	4.580979
234.069624	7209.116401	14.721293	-0.049453	4.578505
234.156059	7201.135959	14.726298	-0.049464	4.576050
233.978837	7193.094686	14.731303	-0.049427	4.573575
233.846923	7185.057690	14.736307	-0.049397	4.571101
233.976957	7177.120417	14.741312	-0.049417	4.568655
233.935885	7169.094837	14.746317	-0.049404	4.566182
233.895115	7161.125242	14.751322	-0.049392	4.563724
234.090154	7153.171125	14.756327	-0.049423	4.561269
234.016799	7145.110170	14.761331	-0.049405	4.558781
233.882159	7137.178207	14.766336	-0.049375	4.556330
233.708612	7129.112410	14.771341	-0.049338	4.553837
233.848107	7121.091955	14.776346	-0.049359	4.551357
233.878087	7113.110681	14.781351	-0.049360	4.548887
233.660976	7105.103793	14.786355	-0.049315	4.546408
233.717171	7097.087772	14.791360	-0.049320	4.543925
233.614640	7089.136438	14.796365	-0.049297	4.541461
233.556693	7081.111703	14.801370	-0.049281	4.538972
233.593731	7073.172305	14.806375	-0.049283	4.536509
233.379093	7065.095018	14.811379	-0.049238	4.534001
233.501468	7057.115572	14.816384	-0.049256	4.531523
233.501046	7049.062934	14.821389	-0.049252	4.529020
233.512604	7041.082926	14.826394	-0.049249	4.526539
233.450622	7033.095777	14.831399	-0.049233	4.524054
233.420890	7025.108805	14.836403	-0.049222	4.521567
233.378051	7017.146383	14.841408	-0.049210	4.519087
233.450963	7009.137398	14.846413	-0.049218	4.516591
233.284059	7001.074636	14.851418	-0.049182	4.514077
233.144105	6993.059240	14.856423	-0.049152	4.511576
233.213219	6984.997643	14.861427	-0.049160	4.509060
233.289545	6977.083366	14.866432	-0.049169	4.506588
233.082925	6969.043006	14.871437	-0.049126	4.504075
233.184560	6961.113315	14.876442	-0.049140	4.501595
233.222944	6953.088765	14.881447	-0.049142	4.499085
233.027796	6945.086782	14.886451	-0.049101	4.496580
233.115284	6937.059789	14.891456	-0.049113	4.494066
233.133515	6929.036927	14.896461	-0.049111	4.491552
233.044252	6921.037523	14.901466	-0.049090	4.489043
233.046700	6913.070571	14.906471	-0.049086	4.486544
232.981149	6905.040149	14.911475	-0.049069	4.484023
232.737570	6897.072759	14.916480	-0.049018	4.481519
232.663559	6889.064438	14.921485	-0.049000	4.479002
232.740151	6881.044152	14.926490	-0.049009	4.476481
232.715889	6873.066168	14.931495	-0.049000	4.473971
232.579331	6865.008660	14.936499	-0.048970	4.471434
232.697754	6857.028212	14.941504	-0.048987	4.468921
232.701038	6849.016895	14.946509	-0.048983	4.466396
232.525804	6841.058721	14.951514	-0.048946	4.463886
232.585485	6833.035040	14.956519	-0.048952	4.461354
232.608805	6825.025234	14.961523	-0.048951	4.458826
232.600788	6817.024307	14.966528	-0.048945	4.456299
232.452037	6809.029683	14.971533	-0.048913	4.453771
232.465375	6800.990236	14.976538	-0.048910	4.451229
232.498227	6793.019250	14.981543	-0.048912	4.448707
232.326641	6784.984465	14.986547	-0.048875	4.446163
232.264393	6777.043552	14.991552	-0.048859	4.443647
232.221297	6769.012378	14.996557	-0.048846	4.441101
232.196322	6761.021015	15.001562	-0.048836	4.438567
232.105174	6753.013509	15.006567	-0.048815	4.436026
232.030750	6744.980910	15.011571	-0.048796	4.433475
232.136962	6736.956299	15.016576	-0.048811	4.430926
232.101189	6728.973663	15.021581	-0.048799	4.428389
231.848611	6720.935004	15.026586	-0.048748	4.425831
231.897883	6713.018247	15.031591	-0.048752	4.423312
231.834717	6704.957703	15.036595	-0.048735	4.420745
231.893410	6696.998965	15.041600	-0.048742	4.418209
231.831303	6688.987894	15.046605	-0.048725	4.415655
231.768689	6680.971712	15.051610	-0.048709	4.413098
231.599219	6672.991230	15.056615	-0.048672	4.410550
231.559594	6664.993816	15.061619	-0.048660	4.407996
231.602873	6656.947951	15.066624	-0.048664	4.405425
231.589684	6648.979936	15.071629	-0.048656	4.402878
231.627289	6640.953263	15.076634	-0.048659	4.400310
231.628184	6633.010863	15.081639	-0.048654	4.397768
231.491852	6624.971111	15.086643	-0.048624	4.395192
231.491018	6616.991277	15.091648	-0.048619	4.392635
231.505342	6608.887352	15.096653	-0.048617	4.390037
231.379773	6600.938538	15.101658	-0.048589	4.387486
231.412466	6592.968269	15.106663	-0.048590	4.384927
231.242481	6585.007244	15.111667	-0.048553	4.382369
231.282648	6576.989848	15.116672	-0.048556	4.379792
231.222732	6569.018782	15.121677	-0.048540	4.377229
231.138899	6560.994662	15.126682	-0.048520	4.374646
231.466611	6553.009323	15.131687	-0.048576	4.372077
231.246455	6544.951694	15.136691	-0.048530	4.369480
231.193143	6536.980006	15.141696	-0.048516	4.366910
231.297650	6528.963557	15.146701	-0.048530	4.364325
231.070497	6521.003721	15.151706	-0.048483	4.361754
231.075484	6513.007390	15.156711	-0.048479	4.359172
231.052892	6504.986406	15.161715	-0.048470	4.356580
231.116294	6496.947253	15.166720	-0.048477	4.353982
230.980296	6488.857098	15.171725	-0.048447	4.351363
231.004390	6480.858274	15.176730	-0.048447	4.348774
231.012119	6472.924291	15.181735	-0.048444	4.346205
230.908590	6464.921239	15.186739	-0.048419	4.343610
230.699806	6456.975273	15.191744	-0.048376	4.341032
230.905843	6448.970505	15.196749	-0.048409	4.338436
230.841833	6440.933928	15.201754	-0.048393	4.335826
230.767925	6432.978332	15.206759	-0.048374	4.333241
230.656131	6424.889124	15.211763	-0.048348	4.330611
230.676456	6416.971824	15.216768	-0.048348	4.328036
230.581600	6408.945748	15.221773	-0.048325	4.325423
230.669872	6400.919517	15.226778	-0.048337	4.322810
230.820304	6392.970462	15.231783	-0.048360	4.320221
230.601888	6384.977068	15.236787	-0.048315	4.317613
230.656155	6376.935470	15.241792	-0.048320	4.314990
230.872627	6368.913165	15.246797	-0.048355	4.312373
230.761375	6360.886089	15.251802	-0.048330	4.309750
230.688328	6352.924168	15.256807	-0.048311	4.307147
230.501164	6344.916358	15.261811	-0.048272	4.304527
230.601315	6336.946699	15.266816	-0.048286	4.301920
230.485185	6328.921279	15.271821	-0.048259	4.299291
230.530810	6320.923566	15.276826	-0.048263	4.296671
230.563401	6312.922471	15.281831	-0.048264	4.294048
230.354877	6304.864654	15.286835	-0.048221	4.291403
230.284941	6296.912092	15.291840	-0.048203	4.288793
230.356720	6288.904793	15.296845	-0.048211	4.286163
230.389859	6280.904310	15.301850	-0.048213	4.283534
230.408239	6272.906261	15.306855	-0.048211	4.280904
230.241245	6264.936848	15.311859	-0.048176	4.278280
230.287828	6256.964986	15.316864	-0.048179	4.275656
230.005029	6248.908055	15.321869	-0.048122	4.272999
230.091525	6240.835215	15.326874	-0.048133	4.270339
230.145140	6232.875161	15.331879	-0.048138	4.267713
230.014219	6224.838853	15.336883	-0.048109	4.265060
229.967465	6216.939537	15.341888	-0.048096	4.262450
229.924908	6208.889147	15.346893	-0.048083	4.259789
229.852342	6200.894647	15.351898	-0.048065	4.257145
229.796897	6192.911285	15.356903	-0.048050	4.254503
229.706870	6184.867881	15.361907	-0.048028	4.251839
229.785036	6176.906849	15.366912	-0.048038	4.249202
229.859424	6168.872700	15.371917	-0.048047	4.246539
229.732672	6160.895330	15.376922	-0.048019	4.243892
229.648557	6152.951876	15.381927	-0.047998	4.241254
229.615105	6144.949940	15.386931	-0.047987	4.238596
229.454141	6136.934169	15.391936	-0.047952	4.235931
229.538194	6128.915491	15.396941	-0.047963	4.233265
229.566321	6120.865012	15.401946	-0.047964	4.230586
229.549042	6112.927810	15.406951	-0.047956	4.227943
229.464894	6104.881406	15.411955	-0.047935	4.225261
229.406301	6096.944237	15.416960	-0.047920	4.222615
229.390626	6088.892917	15.421965	-0.047912	4.219928
229.380567	6080.936320	15.426970	-0.047905	4.217272
229.423905	6072.948560	15.431975	-0.047909	4.214604
229.327845	6064.915004	15.436979	-0.047886	4.211918
229.379095	6056.911961	15.441984	-0.047891	4.209242
229.309230	6048.924260	15.446989	-0.047873	4.206568
229.360972	6040.937897	15.451994	-0.047878	4.203894
229.335341	6032.939460	15.456999	-0.047868	4.201213
228.964749	6024.943028	15.462003	-0.047794	4.198528
228.898457	6016.959917	15.467008	-0.047777	4.195849
229.015970	6008.812488	15.472013	-0.047794	4.193115
228.804570	6000.783049	15.477018	-0.047750	4.190415
229.011482	5992.857731	15.482023	-0.047784	4.187753
229.154693	5984.823470	15.487027	-0.047806	4.185052
228.912795	5976.892198	15.492032	-0.047756	4.182379
228.907281	5968.887004	15.497037	-0.047750	4.179683
228.885814	5960.926400	15.502042	-0.047741	4.176999
229.027859	5952.903503	15.507047	-0.047763	4.174295
228.768499	5944.864009	15.512051	-0.047710	4.171579
228.853930	5936.878360	15.517056	-0.047721	4.168883
228.687146	5928.878657	15.522061	-0.047685	4.166178
228.612725	5920.905086	15.527066	-0.047667	4.163481
228.623708	5912.909820	15.532071	-0.047664	4.160775
228.495180	5904.878460	15.537075	-0.047635	4.158055
228.544139	5896.901556	15.542080	-0.047639	4.155353
228.452557	5888.883156	15.547085	-0.047618	4.152633
228.539518	5880.819662	15.552090	-0.047629	4.149898
228.597498	5872.862679	15.557095	-0.047635	4.147198
228.242460	5864.868483	15.562099	-0.047564	4.144478
228.386082	5856.918907	15.567104	-0.047586	4.141777
228.377930	5848.881707	15.572109	-0.047580	4.139043
228.333508	5840.885054	15.577114	-0.047567	4.136321
228.418983	5832.901832	15.582119	-0.047578	4.133603
228.285333	5824.814571	15.587123	-0.047548	4.130845
228.275477	5816.874673	15.592128	-0.047542	4.128137
228.049794	5808.876578	15.597133	-0.047495	4.125405
228.124073	5800.881051	15.602138	-0.047504	4.122675
228.198207	5792.859748	15.607143	-0.047513	4.119935
228.064277	5784.904443	15.612147	-0.047483	4.117213
228.144838	5776.888058	15.617152	-0.047493	4.114471
227.926903	5768.884577	15.622157	-0.047448	4.111728
227.654915	5760.837573	15.627162	-0.047392	4.108967
227.779426	5752.876594	15.632167	-0.047411	4.106239
227.736521	5744.850850	15.637171	-0.047398	4.103484
227.648135	5736.877716	15.642176	-0.047377	4.100746
227.475885	5728.927722	15.647181	-0.047340	4.098012
227.677033	5720.875124	15.652186	-0.047373	4.095246
227.790430	5712.908420	15.657191	-0.047389	4.092507
227.661635	5704.855870	15.662195	-0.047360	4.089733
227.607339	5696.910999	15.667200	-0.047345	4.086996
227.709509	5688.888336	15.672205	-0.047360	4.084231
227.560179	5680.924495	15.677210	-0.047327	4.081482
227.525569	5672.938902	15.682215	-0.047316	4.078725
227.590653	5664.965569	15.687219	-0.047323	4.075972
227.519090	5656.886643	15.692224	-0.047305	4.073178
227.513374	5648.849424	15.697229	-0.047299	4.070398
227.425847	5640.907595	15.702234	-0.047278	4.067648
227.656708	5632.898683	15.707239	-0.047316	4.064877
227.351363	5624.936096	15.712243	-0.047255	4.062113
227.391097	5616.900023	15.717248	-0.047257	4.059326
227.430372	5608.957596	15.722253	-0.047260	4.056570
227.386575	5600.887439	15.727258	-0.047247	4.053767
227.331796	5592.900573	15.732263	-0.047232	4.050990
227.345467	5584.908255	15.737267	-0.047230	4.048210
227.390945	5576.900355	15.742272	-0.047233	4.045424
227.362547	5568.966512	15.747277	-0.047223	4.042660
227.390056	5560.897823	15.752282	-0.047224	4.039849
227.317695	5552.964306	15.757287	-0.047205	4.037081
227.245737	5544.908374	15.762291	-0.047187	4.034268
226.912232	5536.824726	15.767296	-0.047120	4.031440
226.904139	5528.860457	15.772301	-0.047114	4.028656
226.852084	5520.821524	15.777306	-0.047099	4.025844
226.885401	5512.904878	15.782311	-0.047101	4.023074
226.847362	5504.896122	15.787315	-0.047089	4.020268
226.934700	5496.904355	15.792320	-0.047101	4.017469
226.832152	5488.898084	15.797325	-0.047077	4.014659
226.689033	5480.866375	15.802330	-0.047045	4.011838
226.996507	5472.892176	15.807335	-0.047098	4.009043
226.756259	5464.878793	15.812339	-0.047048	4.006223
226.664570	5456.891068	15.817344	-0.047026	4.003412
226.910496	5448.919396	15.822349	-0.047067	4.000610
226.803538	5440.930300	15.827354	-0.047043	3.997795
226.768641	5432.944472	15.832359	-0.047031	3.994980
226.552672	5424.880588	15.837363	-0.046986	3.992132
226.505930	5416.858073	15.842368	-0.046973	3.989300
226.478870	5408.886316	15.847373	-0.046963	3.986484
226.596414	5400.864918	15.852378	-0.046980	3.983650
226.674428	5392.880147	15.857383	-0.046990	3.980828
226.569792	5384.938680	15.862387	-0.046966	3.978015
226.427459	5376.921833	15.867392	-0.046934	3.975173
226.524055	5368.882753	15.872397	-0.046948	3.972325
226.331021	5360.875480	15.877402	-0.046907	3.969482
226.519378	5352.936727	15.882407	-0.046937	3.966667
226.244572	5344.908866	15.887411	-0.046881	3.963810
226.215265	5336.927785	15.892416	-0.046871	3.960973
226.230661	5328.973972	15.897421	-0.046869	3.958144
225.983031	5320.958816	15.902426	-0.046818	3.955286
226.039878	5312.913722	15.907431	-0.046824	3.952421
225.909935	5304.897576	15.912435	-0.046795	3.949561
225.954499	5296.963589	15.917440	-0.046798	3.946731
226.045233	5288.929859	15.922445	-0.046811	3.943865
225.995677	5280.925470	15.927450	-0.046797	3.941004
225.985894	5272.979936	15.932455	-0.046790	3.938163
225.768683	5264.964129	15.937459	-0.046745	3.935291
225.778523	5256.958604	15.942464	-0.046742	3.932425
225.724497	5248.929029	15.947469	-0.046727	3.929546
225.577606	5240.971838	15.952474	-0.046695	3.926690
225.820716	5232.951201	15.957479	-0.046735	3.923817
225.843682	5224.997928	15.962483	-0.046735	3.920961
225.663284	5217.033024	15.967488	-0.046696	3.918095
225.493783	5209.024010	15.972493	-0.046660	3.915212
225.508521	5200.943875	15.977498	-0.046658	3.912304
225.732580	5192.939535	15.982503	-0.046695	3.909425
225.562916	5184.976965	15.987507	-0.046659	3.906552
225.596841	5176.961304	15.992512	-0.046660	3.903661
225.653465	5168.965085	15.997517	-0.046666	3.900776
225.455388	5160.961313	16.002522	-0.046624	3.897881
225.434168	5152.975006	16.007527	-0.046615	3.894993
225.341009	5144.950984	16.012531	-0.046593	3.892089
225.181888	5136.939937	16.017536	-0.046559	3.889185
225.229938	5128.975623	16.022541	-0.046563	3.886300
225.122723	5121.015156	16.027546	-0.046538	3.883412
225.309286	5113.027746	16.032551	-0.046568	3.880517
224.843876	5105.033100	16.037555	-0.046477	3.877605
224.939910	5096.997237	16.042560	-0.046490	3.874687
225.013598	5088.743782	16.047565	-0.046499	3.871686
224.914284	5080.794185	16.052570	-0.046475	3.868791
225.083652	5072.853944	16.057575	-0.046502	3.865902
225.051653	5064.908319	16.062579	-0.046492	3.863005
225.061327	5056.927890	16.067584	-0.046489	3.860094
225.018861	5048.978579	16.072589	-0.046476	3.857192
224.886304	5040.953122	16.077594	-0.046446	3.854257
224.865234	5032.946439	16.082599	-0.046438	3.851329
224.546092	5024.973527	16.087603	-0.046374	3.848405
224.596770	5016.976800	16.092608	-0.046378	3.845478
224.723414	5009.027877	16.097613	-0.046397	3.842568
224.581905	5000.985119	16.102618	-0.046366	3.839615
224.636787	4993.059982	16.107623	-0.046371	3.836708
224.574333	4985.005583	16.112627	-0.046355	3.833748
224.555896	4977.002480	16.117632	-0.046347	3.830806
224.398944	4969.053303	16.122637	-0.046313	3.827878
224.384894	4960.994454	16.127642	-0.046305	3.824911
224.561908	4953.063047	16.132647	-0.046333	3.821993
224.449075	4945.001115	16.137651	-0.046308	3.819018
224.587876	4937.036703	16.142656	-0.046329	3.816082
224.646347	4929.044147	16.147661	-0.046335	3.813132
224.442399	4921.018971	16.152666	-0.046292	3.810161
224.600673	4913.052425	16.157671	-0.046317	3.807218
224.516233	4905.037046	16.162675	-0.046296	3.804250
224.259838	4897.093664	16.167680	-0.046244	3.801301
224.279519	4889.090631	16.172685	-0.046243	3.798335
224.255591	4881.077079	16.177690	-0.046233	3.795361
224.224438	4873.061848	16.182695	-0.046223	3.792384
223.871715	4865.035109	16.187699	-0.046152	3.789394
223.960533	4857.047251	16.192704	-0.046164	3.786425
223.976222	4849.054910	16.197709	-0.046162	3.783451
224.170037	4841.023803	16.202714	-0.046193	3.780464
224.046246	4833.113540	16.207719	-0.046166	3.777512
223.787090	4825.090556	16.212723	-0.046113	3.774513
223.744321	4817.070972	16.217728	-0.046100	3.771518
223.843289	4809.065027	16.222733	-0.046114	3.768529
223.753905	4801.032666	16.227738	-0.046092	3.765523
223.802536	4793.096703	16.232743	-0.046096	3.762554
223.554367	4785.108568	16.237747	-0.046045	3.759556
223.526369	4777.120011	16.242752	-0.046035	3.756561
223.523112	4769.091395	16.247757	-0.046030	3.753549
223.529181	4761.040394	16.252762	-0.046026	3.750526
223.598493	4753.071678	16.257767	-0.046034	3.747533
223.639052	4745.069606	16.262771	-0.046037	3.744525
223.626763	4737.106281	16.267776	-0.046030	3.741527
223.345985	4729.115665	16.272781	-0.045973	3.738511
223.367041	4721.101857	16.277786	-0.045972	3.735490
223.448879	4713.102269	16.282791	-0.045983	3.732474
223.289901	4705.095447	16.287795	-0.045948	3.729447
223.200808	4697.129573	16.292800	-0.045927	3.726435
223.298475	4689.136000	16.297805	-0.045940	3.723414
223.086436	4681.169504	16.302810	-0.045896	3.720393
223.264671	4673.188666	16.307815	-0.045925	3.717374
223.231383	4665.132362	16.312819	-0.045914	3.714319
223.186161	4657.042356	16.317824	-0.045900	3.711248
223.204213	4649.078239	16.322829	-0.045899	3.708224
223.185895	4641.071249	16.327834	-0.045891	3.705181
223.034122	4633.161579	16.332839	-0.045858	3.702168
222.963073	4625.175273	16.337843	-0.045840	3.699126
222.860871	4617.174680	16.342848	-0.045816	3.696075
222.986570	4609.181323	16.347853	-0.045834	3.693030
222.776512	4601.157752	16.352858	-0.045791	3.689963
222.890897	4593.185694	16.357863	-0.045807	3.686921
222.786370	4585.190592	16.362867	-0.045783	3.683862
222.718885	4577.196458	16.367872	-0.045766	3.680802
222.890214	4569.212651	16.372877	-0.045793	3.677749
222.740934	4561.204716	16.377882	-0.045760	3.674676
222.892848	4553.191497	16.382887	-0.045784	3.671607
222.740835	4545.193154	16.387891	-0.045750	3.668533
222.708288	4537.179725	16.392896	-0.045740	3.665453
222.722459	4529.231571	16.397901	-0.045737	3.662397
222.396427	4521.228785	16.402906	-0.045672	3.659309
222.340539	4513.274489	16.407911	-0.045657	3.656244
222.314420	4505.213150	16.412915	-0.045647	3.653136
222.430982	4497.180475	16.417920	-0.045664	3.650039
222.416069	4489.218539	16.422925	-0.045656	3.646965
222.356014	4481.212334	16.427930	-0.045641	3.643869
222.370279	4473.244951	16.432935	-0.045638	3.640787
222.259446	4465.270393	16.437939	-0.045613	3.637697
222.311399	4457.246273	16.442944	-0.045618	3.634590
222.162073	4449.214026	16.447949	-0.045585	3.631471
222.009764	4441.210669	16.452954	-0.045552	3.628360
222.024912	4433.237882	16.457959	-0.045550	3.625264
222.031771	4425.260447	16.462963	-0.045547	3.622162
222.061462	4417.249748	16.467968	-0.045547	3.619046
222.025196	4409.295461	16.472973	-0.045536	3.615947
221.719383	4401.271806	16.477978	-0.045474	3.612811
221.969036	4393.260669	16.482983	-0.045516	3.609692
222.003188	4385.292448	16.487987	-0.045517	3.606582
221.852558	4377.303541	16.492992	-0.045485	3.603455
221.934297	4369.332153	16.497997	-0.045495	3.600340
221.929553	4361.346732	16.503002	-0.045489	3.597213
221.813599	4353.353156	16.508007	-0.045463	3.594078
221.637612	4345.325584	16.513011	-0.045425	3.590925
221.798587	4337.313395	16.518016	-0.045451	3.587784
221.935775	4329.323380	16.523021	-0.045471	3.584649
221.760112	4321.375721	16.528026	-0.045434	3.581519
221.549212	4313.382949	16.533031	-0.045390	3.578367
221.563621	4305.374527	16.538035	-0.045388	3.575213
221.489666	4297.372517	16.543040	-0.045369	3.572056
221.441093	4289.371802	16.548045	-0.045355	3.568898
221.263951	4281.375019	16.553050	-0.045318	3.565734
221.342802	4273.413099	16.558055	-0.045328	3.562589
221.208543	4265.417161	16.563059	-0.045298	3.559421
221.338525	4257.427715	16.568064	-0.045317	3.556261
221.391547	4249.352629	16.573069	-0.045322	3.553062
221.148951	4241.298976	16.578074	-0.045272	3.549860
221.199744	4233.351793	16.583079	-0.045277	3.546706
221.363127	4225.370244	16.588083	-0.045303	3.543539
221.130268	4217.386316	16.593088	-0.045255	3.540356
221.144731	4209.422395	16.598093	-0.045252	3.537185
221.001185	4201.407855	16.603098	-0.045221	3.533987
220.898987	4193.406115	16.608103	-0.045197	3.530792
220.699548	4185.417488	16.613107	-0.045155	3.527597
220.744894	4177.409752	16.618112	-0.045159	3.524399
220.835800	4169.476791	16.623117	-0.045171	3.521228
220.638112	4161.459209	16.628122	-0.045129	3.518013
220.743215	4153.467104	16.633127	-0.045144	3.514814
220.730701	4145.448482	16.638131	-0.045137	3.511597
220.677709	4137.430230	16.643136	-0.045122	3.508377
220.781758	4129.454609	16.648141	-0.045137	3.505176
220.439181	4121.500657	16.653146	-0.045068	3.501966
220.730885	4113.488617	16.658151	-0.045118	3.498750
220.503413	4105.522686	16.663155	-0.045071	3.495534
220.590374	4097.504061	16.668160	-0.045082	3.492303
220.679441	4089.505025	16.673165	-0.045094	3.489077
220.551383	4081.526518	16.678170	-0.045065	3.485849
220.605242	4073.556593	16.683175	-0.045071	3.482628
220.513447	4065.546912	16.688179	-0.045049	3.479383
220.361339	4057.583404	16.693184	-0.045016	3.476152
220.304101	4049.558302	16.698189	-0.045000	3.472895
220.166825	4041.526356	16.703194	-0.044970	3.469631
220.195682	4033.566384	16.708199	-0.044971	3.466398
220.037764	4025.571184	16.713203	-0.044936	3.463141
220.280695	4017.556886	16.718208	-0.044977	3.459887
220.178062	4009.612190	16.723213	-0.044953	3.456646
220.188379	4001.560328	16.728218	-0.044950	3.453363
219.893817	3993.615597	16.733223	-0.044890	3.450110
219.881063	3985.583191	16.738227	-0.044883	3.446828
219.819418	3977.611996	16.743232	-0.044867	3.443566
220.011113	3969.617921	16.748237	-0.044898	3.440299
219.845283	3961.645203	16.753242	-0.044862	3.437027
219.795178	3953.647900	16.758247	-0.044848	3.433745
219.949918	3945.605807	16.763251	-0.044872	3.430448
219.962698	3937.620971	16.768256	-0.044870	3.427168
220.032685	3929.646668	16.773261	-0.044878	3.423890
219.836568	3921.659432	16.778266	-0.044837	3.420594
219.731435	3913.725483	16.783271	-0.044812	3.417321
219.647971	3905.708140	16.788275	-0.044792	3.414011
219.532767	3897.680088	16.793280	-0.044766	3.410692
219.593862	3889.708676	16.798285	-0.044772	3.407399
219.436013	3881.693790	16.803290	-0.044738	3.404077
219.533897	3873.743066	16.808295	-0.044752	3.400788
219.458308	3865.766330	16.813299	-0.044733	3.397479
219.417817	3857.709486	16.818304	-0.044721	3.394134
219.719059	3849.614608	16.823309	-0.044772	3.390782
219.480040	3841.661665	16.828314	-0.044723	3.387468
219.280434	3833.735789	16.833319	-0.044681	3.384162
219.195591	3825.768343	16.838323	-0.044660	3.380840
219.149856	3817.765046	16.843328	-0.044647	3.377501
219.325258	3809.807706	16.848333	-0.044675	3.374186
219.189777	3801.756887	16.853338	-0.044645	3.370817
219.101193	3793.795232	16.858343	-0.044623	3.367484
219.060937	3785.813517	16.863347	-0.044611	3.364141
218.921690	3777.813255	16.868352	-0.044580	3.360783
219.129009	3769.861183	16.873357	-0.044614	3.357455
219.058546	3761.819712	16.878362	-0.044596	3.354075
218.984676	3753.808204	16.883367	-0.044578	3.350705
219.076826	3745.841596	16.888371	-0.044590	3.347357
218.992678	3737.847834	16.893376	-0.044570	3.343987
218.884549	3729.893863	16.898381	-0.044545	3.340629
218.932308	3721.885562	16.903386	-0.044549	3.337251
218.788312	3713.894709	16.908391	-0.044517	3.333870
218.948002	3705.852989	16.913395	-0.044542	3.330475
218.782667	3697.888446	16.918400	-0.044507	3.327098
218.676151	3689.937948	16.923405	-0.044482	3.323725
218.725198	3681.928170	16.928410	-0.044486	3.320329
218.727310	3673.967453	16.933415	-0.044482	3.316949
218.650082	3665.949931	16.938419	-0.044463	3.313538
218.401603	3657.915557	16.943424	-0.044412	3.310110
218.425496	3649.951866	16.948429	-0.044412	3.306719
218.496909	3641.929167	16.953434	-0.044420	3.303301
218.347546	3633.967344	16.958439	-0.044387	3.299897
218.118380	3626.043588	16.963443	-0.044340	3.296503
218.247728	3618.003315	16.968448	-0.044359	3.293069
218.402350	3609.987318	16.973453	-0.044383	3.289643
218.261233	3602.027339	16.978458	-0.044352	3.286226
218.224094	3594.053237	16.983463	-0.044341	3.282803
218.204955	3586.056058	16.988467	-0.044332	3.279368
218.166616	3578.087881	16.993472	-0.044320	3.275940
218.051509	3570.077035	16.998477	-0.044294	3.272488
217.856453	3562.071114	17.003482	-0.044253	3.269031
217.975505	3554.053072	17.008487	-0.044270	3.265577
217.879660	3546.092726	17.013491	-0.044248	3.262137
217.959440	3538.097312	17.018496	-0.044258	3.258684
217.939543	3530.129578	17.023501	-0.044249	3.255236
217.790354	3522.118076	17.028506	-0.044217	3.251760
217.861205	3514.128759	17.033511	-0.044225	3.248298
217.740745	3506.142590	17.038515	-0.044198	3.244827
217.749922	3498.154468	17.043520	-0.044195	3.241356
217.782363	3490.203587	17.048525	-0.044196	3.237899
217.638645	3482.185838	17.053530	-0.044165	3.234402
217.615345	3474.134843	17.058535	-0.044156	3.230891
217.590324	3466.164271	17.063539	-0.044146	3.227411
217.574149	3458.173628	17.068544	-0.044138	3.223920
217.641544	3450.213785	17.073549	-0.044146	3.220441
217.467168	3442.227488	17.078554	-0.044109	3.216937
217.154323	3434.259448	17.083559	-0.044046	3.213432
217.233448	3426.219216	17.088563	-0.044056	3.209907
217.310422	3418.246937	17.093568	-0.044065	3.206409
217.331463	3410.282234	17.098573	-0.044065	3.202907
217.072457	3402.276253	17.103578	-0.044011	3.199372
217.083937	3394.318674	17.108583	-0.044009	3.195865
217.085164	3386.326248	17.113587	-0.044004	3.192339
217.119239	3378.297843	17.118592	-0.044006	3.188794
217.153184	3370.306587	17.123597	-0.044007	3.185262
216.953168	3362.348009	17.128602	-0.043965	3.181730
216.799531	3354.372090	17.133607	-0.043932	3.178189
216.947955	3346.375374	17.138611	-0.043955	3.174647
216.852492	3338.380815	17.143616	-0.043932	3.171092
216.868148	3330.390151	17.148621	-0.043930	3.167540
216.756790	3322.393404	17.153626	-0.043905	3.163975
216.873496	3314.431915	17.158631	-0.043922	3.160432
216.740325	3306.454628	17.163635	-0.043892	3.156867
216.782863	3298.440673	17.168640	-0.043895	3.153289
216.756569	3290.436927	17.173645	-0.043886	3.149709
216.584380	3282.462135	17.178650	-0.043849	3.146131
216.704245	3274.458845	17.183655	-0.043866	3.142549
216.443214	3266.507567	17.188659	-0.043813	3.138969
216.607055	3258.500096	17.193664	-0.043839	3.135380
216.476008	3250.507183	17.198669	-0.043810	3.131779
216.274369	3242.525648	17.203674	-0.043767	3.128176
216.427725	3234.527294	17.208679	-0.043791	3.124577
216.572662	3226.583853	17.213683	-0.043813	3.120999
216.321186	3218.612163	17.218688	-0.043762	3.117386
216.120373	3210.619281	17.223693	-0.043720	3.113761
216.282368	3202.570017	17.228698	-0.043745	3.110123
216.135048	3194.600898	17.233703	-0.043713	3.106503
216.132903	3186.643798	17.238707	-0.043708	3.102891
215.966930	3178.667082	17.243712	-0.043672	3.099258
216.195878	3170.680703	17.248717	-0.043710	3.095635
215.939683	3162.694856	17.253722	-0.043657	3.091985
215.902146	3154.677364	17.258727	-0.043646	3.088327
216.028642	3146.680835	17.263731	-0.043664	3.084681
215.979547	3138.724438	17.268736	-0.043650	3.081042
215.975531	3130.755173	17.273741	-0.043645	3.077394
216.035847	3122.707120	17.278746	-0.043651	3.073709
215.910190	3114.671302	17.283751	-0.043623	3.070016
215.844942	3106.726675	17.288755	-0.043606	3.066364
215.646368	3098.760399	17.293760	-0.043564	3.062691
215.845381	3090.771204	17.298765	-0.043597	3.059021
215.554450	3082.814682	17.303770	-0.043538	3.055339
215.658225	3074.827334	17.308775	-0.043552	3.051658
215.636017	3066.831490	17.313779	-0.043543	3.047962
215.526490	3058.828066	17.318784	-0.043518	3.044253
215.303430	3050.918923	17.323789	-0.043472	3.040579
215.176973	3042.946893	17.328794	-0.043444	3.036875
215.349882	3034.908584	17.333799	-0.043471	3.033150
215.501303	3026.886319	17.338803	-0.043494	3.029428
215.283108	3018.919697	17.343808	-0.043449	3.025709
215.356501	3010.952647	17.348813	-0.043458	3.021999
215.319058	3002.975505	17.353818	-0.043446	3.018274
215.209141	2994.993782	17.358823	-0.043421	3.014539
215.155384	2986.992109	17.363827	-0.043406	3.010793
215.194725	2978.993304	17.368832	-0.043409	3.007048
215.165572	2971.035603	17.373837	-0.043399	3.003315
214.953639	2963.068556	17.378842	-0.043354	2.999563
215.152734	2955.093370	17.383847	-0.043387	2.995823
214.894679	2947.077686	17.388851	-0.043334	2.992037
214.843060	2939.071571	17.393856	-0.043319	2.988260
215.028100	2931.077563	17.398861	-0.043349	2.984497
214.975711	2923.111552	17.403866	-0.043335	2.980730
214.862507	2915.170696	17.408871	-0.043309	2.976967
214.897698	2907.182597	17.413875	-0.043310	2.973184
214.630612	2899.179775	17.418880	-0.043256	2.969374
214.489158	2891.233669	17.423885	-0.043225	2.965593
214.554613	2883.236843	17.428890	-0.043232	2.961793
214.504243	2875.255501	17.433895	-0.043218	2.957990
214.569768	2867.275884	17.438899	-0.043226	2.954189
214.254187	2859.273813	17.443904	-0.043162	2.950352
214.393444	2851.291197	17.448909	-0.043183	2.946543
214.443981	2843.289990	17.453914	-0.043188	2.942716
214.329390	2835.311233	17.458919	-0.043162	2.938886
214.306257	2827.355094	17.463923	-0.043153	2.935066
214.203197	2819.345316	17.468928	-0.043129	2.931212
214.191492	2811.372467	17.473933	-0.043122	2.927375
214.073384	2803.402932	17.478938	-0.043095	2.923529
214.285844	2795.411620	17.483943	-0.043130	2.919685
214.276349	2787.488656	17.488947	-0.043123	2.915857
214.077333	2779.401504	17.493952	-0.043081	2.911935
214.109427	2771.415202	17.498957	-0.043083	2.908068
213.970669	2763.447414	17.503962	-0.043052	2.904196
213.824861	2755.502667	17.508967	-0.043020	2.900330
213.971302	2747.533677	17.513971	-0.043043	2.896462
213.953726	2739.516558	17.518976	-0.043034	2.892557
213.636945	2731.565260	17.523981	-0.042971	2.888663
213.530462	2723.575259	17.528986	-0.042946	2.884756
213.733942	2715.604980	17.533991	-0.042979	2.880870
213.590946	2707.657903	17.538995	-0.042948	2.876971
213.551047	2699.641420	17.544000	-0.042936	2.873039
213.774337	2691.624876	17.549005	-0.042972	2.869115
213.729499	2683.642287	17.554010	-0.042959	2.865188
213.563622	2675.712788	17.559015	-0.042924	2.861275
213.561888	2667.758021	17.564019	-0.042919	2.857354
213.605952	2659.719898	17.569024	-0.042922	2.853388
213.518701	2651.736794	17.574029	-0.042901	2.849437
213.366240	2643.799289	17.579034	-0.042868	2.845499
213.388728	2635.832877	17.584039	-0.042867	2.841552
213.375965	2627.877756	17.589043	-0.042860	2.837602
213.240201	2619.862985	17.594048	-0.042830	2.833610
213.228567	2611.854835	17.599053	-0.042823	2.829623
212.991994	2603.891791	17.604058	-0.042774	2.825640
212.775042	2595.936609	17.609063	-0.042729	2.821656
212.876339	2587.953829	17.614067	-0.042743	2.817671
213.044991	2579.934052	17.619072	-0.042770	2.813666
212.856623	2571.970987	17.624077	-0.042730	2.809663
212.749908	2564.009973	17.629082	-0.042705	2.805660
212.783990	2556.031731	17.634087	-0.042707	2.801651
212.834187	2548.075420	17.639091	-0.042712	2.797648
212.539086	2540.082560	17.644096	-0.042652	2.793600
212.652027	2532.081339	17.649101	-0.042668	2.789567
212.575662	2524.109284	17.654106	-0.042649	2.785531
212.563785	2516.140708	17.659111	-0.042642	2.781495
212.509288	2508.170828	17.664115	-0.042627	2.777450
212.449294	2500.199716	17.669120	-0.042611	2.773398
212.566502	2492.184617	17.674125	-0.042628	2.769328
212.460010	2484.227014	17.679130	-0.042604	2.765268
212.473859	2476.281110	17.684135	-0.042602	2.761215
212.389250	2468.329114	17.689139	-0.042581	2.757148
212.121072	2460.301351	17.694144	-0.042526	2.753024
212.140698	2452.269511	17.699149	-0.042525	2.748910
212.329333	2444.258915	17.704154	-0.042555	2.744810
212.194178	2436.347010	17.709159	-0.042526	2.740736
211.884452	2428.430641	17.714163	-0.042463	2.736642
212.161796	2420.374972	17.719168	-0.042510	2.732506
212.332303	2412.386326	17.724173	-0.042537	2.728392
212.007622	2404.454064	17.729178	-0.042472	2.724271
212.002377	2396.484474	17.734183	-0.042466	2.720144
212.150744	2388.533908	17.739187	-0.042489	2.716030
211.913201	2380.541140	17.744192	-0.042440	2.711863
211.829209	2372.569984	17.749197	-0.042419	2.707711
211.848426	2364.587344	17.754202	-0.042418	2.703553
211.647226	2356.630297	17.759207	-0.042376	2.699389
211.678940	2348.685073	17.764211	-0.042377	2.695238
211.628551	2340.664222	17.769216	-0.042363	2.691037
211.674848	2332.706731	17.774221	-0.042367	2.686868
211.673781	2324.733421	17.779226	-0.042362	2.682681
211.637415	2316.778016	17.784231	-0.042350	2.678495
211.800447	2308.799627	17.789235	-0.042376	2.674303
211.486855	2300.782749	17.794240	-0.042313	2.670054
211.402489	2292.843607	17.799245	-0.042292	2.665854
211.388288	2284.865443	17.804250	-0.042285	2.661631
211.381343	2276.894941	17.809255	-0.042279	2.657405
211.355989	2268.937015	17.814259	-0.042269	2.653179
211.366633	2260.918737	17.819264	-0.042267	2.648916
211.294787	2252.965642	17.824269	-0.042248	2.644675
211.108229	2245.039138	17.829274	-0.042209	2.640434
210.996769	2237.086460	17.834279	-0.042183	2.636177
210.984150	2229.075350	17.839283	-0.042176	2.631889
210.938935	2221.073467	17.844288	-0.042163	2.627597
210.883421	2213.139401	17.849293	-0.042148	2.623333
210.860766	2205.151555	17.854298	-0.042139	2.619035
210.925665	2197.163657	17.859303	-0.042146	2.614736
210.932441	2189.195203	17.864307	-0.042143	2.610437
210.703296	2181.243238	17.869312	-0.042095	2.606124
210.933479	2173.293158	17.874317	-0.042134	2.601835
210.676908	2165.332500	17.879322	-0.042081	2.597501
210.701741	2157.264840	17.884327	-0.042081	2.593120
210.812995	2149.176760	17.889331	-0.042097	2.588727
210.568456	2141.244222	17.894336	-0.042046	2.584387
210.663534	2133.331653	17.899341	-0.042059	2.580073
210.585936	2125.397495	17.904346	-0.042040	2.575729
210.646187	2117.405311	17.909351	-0.042047	2.571355
210.581314	2109.458379	17.914355	-0.042030	2.566990
210.406363	2101.516768	17.919360	-0.041992	2.562612
210.404150	2093.571508	17.924365	-0.041987	2.558238
210.508580	2085.591827	17.929370	-0.042002	2.553844
210.448008	2077.598475	17.934375	-0.041986	2.549423
210.486242	2069.639431	17.939379	-0.041988	2.545021
210.424644	2061.692205	17.944384	-0.041972	2.540610
210.202211	2053.761056	17.949389	-0.041926	2.536190
210.137367	2045.775814	17.954394	-0.041909	2.531742
210.114173	2037.784760	17.959399	-0.041900	2.527287
210.105673	2029.839164	17.964403	-0.041894	2.522850
209.943661	2021.890978	17.969408	-0.041859	2.518393
209.834280	2013.943238	17.974413	-0.041834	2.513932
209.731732	2005.929323	17.979418	-0.041810	2.509426
209.590614	1997.962004	17.984423	-0.041779	2.504936
209.753044	1990.013084	17.989427	-0.041804	2.500470
209.629841	1982.047174	17.994432	-0.041776	2.495966
209.706426	1974.051660	17.999437	-0.041786	2.491451
209.649918	1966.094986	18.004442	-0.041771	2.486940
209.758392	1958.127519	18.009447	-0.041786	2.482427
209.602438	1950.229679	18.014451	-0.041752	2.477926
209.452436	1942.248286	18.019456	-0.041720	2.473370
209.431377	1934.253400	18.024461	-0.041711	2.468807
209.317018	1926.298302	18.029466	-0.041685	2.464251
209.197591	1918.346384	18.034471	-0.041658	2.459689
209.437623	1910.374190	18.039475	-0.041698	2.455133
209.273420	1902.415639	18.044480	-0.041662	2.450546
209.222747	1894.460969	18.049485	-0.041648	2.445961
209.206642	1886.502906	18.054490	-0.041641	2.441369
209.162159	1878.553573	18.059495	-0.041627	2.436770
208.989989	1870.573363	18.064499	-0.041591	2.432136
208.789512	1862.567051	18.069504	-0.041549	2.427475
208.951955	1854.599319	18.074509	-0.041574	2.422855
208.888225	1846.655209	18.079514	-0.041557	2.418223
208.852570	1838.691095	18.084519	-0.041546	2.413572
208.688238	1830.739702	18.089523	-0.041511	2.408910
208.581704	1822.786793	18.094528	-0.041486	2.404243
208.613929	1814.845245	18.099533	-0.041487	2.399584
208.547181	1806.910023	18.104538	-0.041470	2.394911
208.530512	1798.918265	18.109543	-0.041462	2.390201
208.542831	1790.960304	18.114547	-0.041460	2.385503
208.296274	1783.012888	18.119552	-0.041409	2.380781
208.406331	1775.064838	18.124557	-0.041425	2.376078
208.415787	1767.086626	18.129562	-0.041422	2.371340
208.139454	1759.143413	18.134567	-0.041366	2.366591
208.288764	1751.178043	18.139571	-0.041389	2.361852
208.304640	1743.222026	18.144576	-0.041387	2.357099
208.118320	1735.279932	18.149581	-0.041347	2.352329
207.962982	1727.311143	18.154586	-0.041314	2.347535
208.174982	1719.316458	18.159591	-0.041348	2.342746
208.241412	1711.385422	18.164595	-0.041356	2.337973
208.060778	1703.428162	18.169600	-0.041318	2.333155
208.102885	1695.477753	18.174605	-0.041321	2.328349
208.104224	1687.513263	18.179610	-0.041316	2.323521
207.847120	1679.614962	18.184615	-0.041264	2.318702
207.736409	1671.680443	18.189619	-0.041238	2.313863
207.796130	1663.667425	18.194624	-0.041245	2.308980
207.783469	1655.713366	18.199629	-0.041238	2.304116
207.733487	1647.793181	18.204634	-0.041224	2.299260
207.404473	1639.863839	18.209639	-0.041158	2.294365
207.542114	1631.879033	18.214643	-0.041178	2.289464
207.372226	1623.942983	18.219648	-0.041142	2.284557
207.284621	1616.016261	18.224653	-0.041121	2.279652
207.241014	1608.063545	18.229658	-0.041108	2.274724
207.208038	1600.008006	18.234663	-0.041097	2.269723
207.050089	1592.088842	18.239667	-0.041063	2.264784
207.213217	1584.112961	18.244672	-0.041089	2.259827
207.199941	1576.192200	18.249677	-0.041081	2.254878
207.091509	1568.235066	18.254682	-0.041056	2.249888
207.036056	1560.276333	18.259687	-0.041041	2.244890
207.203044	1552.342738	18.264691	-0.041068	2.239916
206.851296	1544.441483	18.269696	-0.040997	2.234905
206.866095	1536.463679	18.274701	-0.040995	2.229868
206.915770	1528.506625	18.279706	-0.041000	2.224835
206.872596	1520.565318	18.284711	-0.040987	2.219792
206.747642	1512.657974	18.289715	-0.040959	2.214753
206.732091	1504.668669	18.294720	-0.040952	2.209659
206.846276	1496.716349	18.299725	-0.040968	2.204589
206.627905	1488.822332	18.304730	-0.040923	2.199514
206.549055	1480.886631	18.309735	-0.040903	2.194414
206.626983	1472.896342	18.314739	-0.040913	2.189281
206.295974	1464.968149	18.319744	-0.040847	2.184138
206.427323	1457.014721	18.324749	-0.040866	2.179009
206.438099	1449.071045	18.329754	-0.040864	2.173864
206.436927	1441.112798	18.334759	-0.040859	2.168695
206.379681	1433.187241	18.339763	-0.040843	2.163531
206.151922	1425.280819	18.344768	-0.040796	2.158351
206.008850	1417.355211	18.349773	-0.040765	2.153153
206.091563	1409.375398	18.354778	-0.040775	2.147929
205.938284	1401.446820	18.359783	-0.040742	2.142703
206.087437	1393.504007	18.364787	-0.040765	2.137483
206.021520	1385.555879	18.369792	-0.040748	2.132227
205.703859	1377.653687	18.374797	-0.040684	2.126965
205.913383	1369.685497	18.379802	-0.040718	2.121696
205.751508	1361.765403	18.384807	-0.040684	2.116410
205.968598	1353.746454	18.389811	-0.040719	2.111081
205.803830	1345.814421	18.394816	-0.040684	2.105760
205.622009	1337.926863	18.399821	-0.040645	2.100454
205.552149	1330.005087	18.404826	-0.040627	2.095122
205.421353	1322.060301	18.409831	-0.040598	2.089755
205.479298	1314.120801	18.414835	-0.040604	2.084397
205.473662	1306.195483	18.419840	-0.040599	2.079028
205.178550	1298.302957	18.424845	-0.040539	2.073638
205.261231	1290.332304	18.429850	-0.040550	2.068219
205.279537	1282.385465	18.434855	-0.040548	2.062796
205.384302	1274.459593	18.439859	-0.040563	2.057381
205.139310	1266.551654	18.444864	-0.040513	2.051929
205.040871	1258.621201	18.449869	-0.040490	2.046462
204.931183	1250.716130	18.454874	-0.040464	2.040996
204.961146	1242.784719	18.459879	-0.040465	2.035512
205.005055	1234.813484	18.464883	-0.040469	2.029987
205.083240	1226.846960	18.469888	-0.040478	2.024453
204.856023	1218.987886	18.474893	-0.040431	2.018948
204.730836	1211.072247	18.479898	-0.040403	2.013398
204.777736	1203.114806	18.484903	-0.040407	2.007822
204.815382	1195.196069	18.489907	-0.040410	2.002257
204.618612	1187.305565	18.494912	-0.040368	1.996671
204.670958	1179.349126	18.499917	-0.040373	1.991049
204.819742	1171.399201	18.504922	-0.040396	1.985427
204.710501	1163.501098	18.509927	-0.040371	1.979797
204.578658	1155.623645	18.514931	-0.040342	1.974164
204.429658	1147.685246	18.519936	-0.040309	1.968470
204.345319	1139.775666	18.524941	-0.040289	1.962786
204.380518	1131.867670	18.529946	-0.040291	1.957100
204.348885	1123.892394	18.534951	-0.040280	1.951341
204.322143	1115.956717	18.539955	-0.040270	1.945595
204.108607	1108.066108	18.544960	-0.040226	1.939844
204.263537	1100.134387	18.549965	-0.040250	1.934086
203.988598	1092.241805	18.554970	-0.040194	1.928293
204.005215	1084.305958	18.559975	-0.040193	1.922482
204.104795	1076.402313	18.564979	-0.040206	1.916686
204.078815	1068.473340	18.569984	-0.040197	1.910841
204.070812	1060.565685	18.574989	-0.040191	1.904995
204.092683	1052.670596	18.579994	-0.040190	1.899144
203.905217	1044.771843	18.584999	-0.040150	1.893248
203.815322	1036.862929	18.590003	-0.040129	1.887338
203.769109	1028.966352	18.595008	-0.040116	1.881423
203.768169	1021.069234	18.600013	-0.040111	1.875494
203.823638	1013.118293	18.605018	-0.040116	1.869512
203.555799	1005.233446	18.610023	-0.040062	1.863524
203.588741	997.341490	18.615027	-0.040063	1.857546
203.561360	989.416277	18.620032	-0.040053	1.851516
203.520579	981.509523	18.625037	-0.040041	1.845479
203.485328	973.632267	18.630042	-0.040030	1.839445
203.449315	965.733276	18.635047	-0.040018	1.833375
203.398512	957.823273	18.640051	-0.040004	1.827274
203.135822	949.956622	18.645056	-0.039950	1.821161
203.236102	942.039875	18.650061	-0.039964	1.815033
203.309597	934.118635	18.655066	-0.039973	1.808876
202.919486	926.279804	18.660071	-0.039896	1.802707
202.891672	918.403453	18.665075	-0.039886	1.796531
202.963228	910.422439	18.670080	-0.039895	1.790264
202.856247	902.537459	18.675085	-0.039870	1.784028
202.639963	894.690791	18.680090	-0.039825	1.777788
202.650581	886.777297	18.685095	-0.039822	1.771500
202.613814	878.891408	18.690099	-0.039811	1.765207
202.541457	871.016795	18.695104	-0.039793	1.758895
202.553785	863.116307	18.700109	-0.039790	1.752550
202.498864	855.215072	18.705114	-0.039775	1.746173
202.375640	847.352433	18.710119	-0.039748	1.739796
202.383855	839.481965	18.715123	-0.039744	1.733405
202.215359	831.604743	18.720128	-0.039708	1.726962
202.090599	823.739295	18.725133	-0.039680	1.720511
201.823729	815.899218	18.730138	-0.039626	1.714038
201.979629	807.952242	18.735143	-0.039650	1.707506
201.997168	800.082513	18.740147	-0.039649	1.700996
201.806793	792.228601	18.745152	-0.039609	1.694447
201.670639	784.355140	18.750157	-0.039579	1.687862
201.671521	776.483711	18.755162	-0.039574	1.681272
201.609732	768.621137	18.760167	-0.039558	1.674655
201.476632	760.750927	18.765171	-0.039528	1.667996
201.519348	752.858358	18.770176	-0.039532	1.661315
201.296521	745.032531	18.775181	-0.039486	1.654628
201.352612	737.150858	18.780186	-0.039491	1.647903
201.483183	729.262474	18.785191	-0.039511	1.641156
201.506094	721.414652	18.790195	-0.039510	1.634401
201.176007	713.537257	18.795200	-0.039444	1.627543
201.090046	705.687278	18.800205	-0.039424	1.620714
201.049360	697.850646	18.805210	-0.039411	1.613874
200.780279	689.998653	18.810215	-0.039357	1.606960
200.813590	682.158493	18.815219	-0.039358	1.600068
200.790980	674.307567	18.820224	-0.039349	1.593130
200.756900	666.447524	18.825229	-0.039338	1.586151
200.757961	658.607107	18.830234	-0.039334	1.579164
200.828566	650.740676	18.835239	-0.039342	1.572133
200.749272	642.916692	18.840243	-0.039323	1.565086
200.491661	635.126098	18.845248	-0.039270	1.558012
200.364780	627.282984	18.850253	-0.039242	1.550877
200.387400	619.428382	18.855258	-0.039241	1.543720
200.169487	611.605427	18.860263	-0.039196	1.536523
200.236020	603.764601	18.865267	-0.039204	1.529319
200.185443	595.932275	18.870272	-0.039190	1.522070
200.017094	588.140480	18.875277	-0.039154	1.514807
199.933338	580.318811	18.880282	-0.039133	1.507494
199.680819	572.517825	18.885287	-0.039082	1.500139
199.921938	564.669503	18.890291	-0.039122	1.492778
199.693825	556.864118	18.895296	-0.039075	1.485349
199.739090	549.059222	18.900301	-0.039079	1.477926
199.743679	541.206647	18.905306	-0.039075	1.470414
199.428026	533.419473	18.910311	-0.039011	1.462875
199.433535	525.618319	18.915315	-0.039008	1.455335
199.635615	517.763608	18.920320	-0.039041	1.447734
199.401435	510.014964	18.925325	-0.038992	1.440127
199.124799	502.262921	18.930330	-0.038936	1.432470
199.232050	494.420429	18.935335	-0.038952	1.424744
199.347965	486.632742	18.940339	-0.038968	1.417032
198.980435	478.887813	18.945344	-0.038895	1.409241
198.902874	471.111501	18.950349	-0.038876	1.401423
199.054630	463.311834	18.955354	-0.038900	1.393576
198.916248	455.520994	18.960359	-0.038870	1.385644
198.809222	447.779967	18.965363	-0.038845	1.377724
198.699811	440.005344	18.970368	-0.038820	1.369722
198.721290	432.226022	18.975373	-0.038819	1.361691
198.519862	424.513730	18.980378	-0.038777	1.353643
198.360064	416.748612	18.985383	-0.038743	1.345499
198.320018	409.013888	18.990387	-0.038731	1.337359
198.004823	401.286688	18.995392	-0.038667	1.329128
197.932242	393.535857	19.000397	-0.038649	1.320863
198.016216	385.738371	19.005402	-0.038660	1.312525
197.852475	377.928353	19.010407	-0.038625	1.304075
197.896228	370.199949	19.015411	-0.038629	1.295696
197.680387	362.496337	19.020416	-0.038584	1.287242
197.732885	354.773143	19.025421	-0.038589	1.278761
197.711868	347.065614	19.030426	-0.038581	1.270226
197.379252	339.390737	19.035431	-0.038514	1.261612
197.431198	331.683066	19.040435	-0.038519	1.252974
197.253158	323.995187	19.045440	-0.038481	1.244255
197.000070	316.341865	19.050445	-0.038430	1.235498
197.099970	308.604731	19.055450	-0.038444	1.226652
197.241813	300.886475	19.060455	-0.038466	1.217772
197.030188	293.243431	19.065459	-0.038422	1.208844
196.830240	285.598428	19.070464	-0.038380	1.199850
196.601886	277.962920	19.075469	-0.038333	1.190793
196.616928	270.290071	19.080474	-0.038331	1.181672
196.420804	262.660424	19.085479	-0.038290	1.172488
196.509865	254.992344	19.090483	-0.038302	1.163244
196.353825	247.369990	19.095488	-0.038268	1.153931
195.972045	239.752044	19.100493	-0.038193	1.144499
196.125425	232.098565	19.105498	-0.038217	1.135059
196.074534	224.471968	19.110503	-0.038203	1.125530
195.794453	216.918218	19.115507	-0.038146	1.115962
195.719709	209.310240	19.120512	-0.038128	1.106286
195.399221	201.770508	19.125517	-0.038063	1.096558
195.350006	194.177617	19.130522	-0.038050	1.086735
195.245869	186.621580	19.135527	-0.038026	1.076859
195.375593	179.016362	19.140531	-0.038045	1.066879
195.313723	171.465138	19.145536	-0.038029	1.056832
194.875530	163.976626	19.150541	-0.037943	1.046686
194.879842	156.450042	19.155546	-0.037940	1.036493
194.693713	148.943793	19.160551	-0.037901	1.026182
194.769069	141.422902	19.165555	-0.037910	1.015808
194.463661	133.961034	19.170560	-0.037849	1.005317
194.286402	126.499135	19.175565	-0.037811	0.994747
194.452249	118.955086	19.180570	-0.037838	0.984031
193.848300	111.586019	19.185575	-0.037721	0.973256
193.880426	104.121873	19.190579	-0.037723	0.962384
193.938938	96.678996	19.195584	-0.037729	0.951426
193.682915	89.295288	19.200589	-0.037677	0.940347
193.475186	81.923713	19.205594	-0.037634	0.929166
193.153374	74.586424	19.210599	-0.037570	0.917871
193.030082	67.222354	19.215603	-0.037542	0.906448
192.826805	60.124373	19.220608	-0.037500	0.895276