Fri Mar 12 12:41:22 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.716197	0.003158	0.000000	0.000005	0.722689

0.647863	0.012245	0.005005	0.000018	0.722684
0.686275	-0.082172	0.010010	0.000010	0.722512
0.862471	-0.189734	0.015014	-0.000022	0.722362
0.891851	-0.191565	0.020019	-0.000028	0.722369
0.725935	-0.162240	0.025024	0.000003	0.722369
0.734393	-0.166905	0.030029	0.000001	0.722363
0.700654	-0.157139	0.035034	0.000007	0.722371
0.866112	-0.191548	0.040038	-0.000024	0.722361
0.919532	-0.198773	0.045043	-0.000034	0.722366
0.863065	-0.186114	0.050048	-0.000023	0.722371
0.861250	-0.188751	0.055053	-0.000023	0.722366
0.732943	-0.161670	0.060058	0.000001	0.722374
0.913187	-0.198274	0.065062	-0.000033	0.722365
0.821871	-0.181119	0.070067	-0.000016	0.722367
0.821283	-0.255598	0.075072	-0.000016	0.722221
0.879520	-0.344351	0.080077	-0.000027	0.722067
0.850635	-0.334776	0.085082	-0.000022	0.722076
0.729419	-0.318098	0.090086	0.000001	0.722067
0.810248	-0.328774	0.095091	-0.000014	0.722074
0.901420	-0.346537	0.100096	-0.000031	0.722071
0.665923	-0.328025	0.105101	0.000012	0.722026
0.657476	-0.467084	0.110106	0.000014	0.721750
0.557493	-0.455178	0.115110	0.000033	0.721738
0.692727	-0.477251	0.120115	0.000007	0.721742
0.785346	-0.492690	0.125120	-0.000010	0.721745
0.502569	-0.445612	0.130125	0.000042	0.721738
0.575352	-0.596817	0.135130	0.000029	0.721467
0.410106	-0.584839	0.140134	0.000060	0.721433
0.645270	-0.623716	0.145139	0.000016	0.721439
0.674566	-0.629427	0.150144	0.000010	0.721438
0.414675	-0.667082	0.155149	0.000058	0.721273
0.596394	-0.774983	0.160154	0.000025	0.721125
0.596707	-0.780494	0.165158	0.000024	0.721114
0.691501	-0.795131	0.170163	0.000007	0.721119
0.535898	-0.851200	0.175168	0.000036	0.720954
0.400283	-0.870231	0.180173	0.000061	0.720870
0.581795	-0.899756	0.185178	0.000027	0.720875
0.449853	-0.908131	0.190182	0.000051	0.720813
0.573835	-1.071687	0.195187	0.000028	0.720534
0.690447	-1.090331	0.200192	0.000006	0.720539
0.368724	-1.038846	0.205197	0.000066	0.720528
0.156148	-1.156241	0.210202	0.000106	0.720222
0.192663	-1.166092	0.215206	0.000099	0.720216
0.312668	-1.187006	0.220211	0.000076	0.720217
0.451793	-1.357302	0.225216	0.000051	0.719930
0.433502	-1.373871	0.230221	0.000054	0.719891
0.249725	-1.350985	0.235226	0.000088	0.719872
0.014071	-1.449437	0.240230	0.000132	0.719596
0.094497	-1.462869	0.245235	0.000117	0.719598
0.355091	-1.561920	0.250240	0.000068	0.719494
0.229221	-1.659625	0.255245	0.000092	0.719257
0.388267	-1.682982	0.260250	0.000062	0.719267
0.268964	-1.789218	0.265254	0.000084	0.719016
0.248059	-1.815781	0.270259	0.000088	0.718957
0.195049	-1.862691	0.275264	0.000098	0.718846
-0.138417	-1.909354	0.280269	0.000160	0.718637
0.030715	-1.934514	0.285274	0.000128	0.718647
-0.220588	-2.032505	0.290278	0.000175	0.718365
-0.104309	-2.060942	0.295283	0.000153	0.718350
0.029993	-2.184679	0.300288	0.000128	0.718153
-0.735753	-2.119672	0.305293	0.000270	0.718012
-0.981441	-2.101375	0.310298	0.000316	0.717962
-1.696124	-2.108396	0.315302	0.000449	0.717697
-2.236316	-2.010698	0.320307	0.000550	0.717700
-1.936989	-2.117025	0.325312	0.000494	0.717595
-2.800481	-2.073585	0.330317	0.000654	0.717377
-2.710748	-2.087061	0.335322	0.000638	0.717383
-3.065949	-2.059928	0.340326	0.000704	0.717311
-3.468236	-2.103759	0.345331	0.000778	0.717083
-3.423529	-2.111228	0.350336	0.000770	0.717084
-4.168184	-1.982237	0.355341	0.000908	0.717077
-3.959934	-2.149963	0.360346	0.000870	0.716819
-4.862169	-2.025395	0.365350	0.001038	0.716748
-5.249742	-1.954997	0.370355	0.001110	0.716751
-4.595912	-2.069036	0.375360	0.000988	0.716756
-5.088046	-2.109854	0.380365	0.001079	0.716501
-5.800550	-2.008736	0.385370	0.001212	0.716451
-5.503871	-2.064007	0.390374	0.001157	0.716446
-5.418284	-2.079272	0.395379	0.001141	0.716446
-5.714164	-2.104982	0.400384	0.001196	0.716291
-6.738909	-2.006786	0.405389	0.001386	0.716124
-5.894469	-2.151674	0.410394	0.001229	0.716135
-6.182586	-2.103995	0.415398	0.001282	0.716128
-6.697787	-2.012081	0.420403	0.001378	0.716129
-6.858527	-2.092747	0.425408	0.001408	0.715912
-7.343784	-2.024205	0.430413	0.001498	0.715877
-7.351708	-2.019189	0.435418	0.001500	0.715884
-7.158616	-2.057899	0.440422	0.001464	0.715876
-7.365120	-2.019871	0.445427	0.001502	0.715879
-7.251866	-2.175175	0.450432	0.001481	0.715611
-8.456513	-1.998035	0.455437	0.001705	0.715537
-8.046061	-2.067119	0.460442	0.001628	0.715545
-8.102537	-2.060305	0.465446	0.001639	0.715539
-8.425516	-2.002631	0.470451	0.001699	0.715539
-8.146486	-2.101444	0.475456	0.001647	0.715442
-9.124566	-2.037614	0.480461	0.001829	0.715223
-8.885227	-2.076414	0.485466	0.001784	0.715231
-9.202094	-2.024746	0.490470	0.001843	0.715222
-8.971582	-2.064336	0.495475	0.001800	0.715225
-8.893913	-2.076814	0.500480	0.001786	0.715228
-9.362642	-2.072059	0.505485	0.001873	0.715072
-10.058763	-2.033303	0.510490	0.002002	0.714903
-9.670366	-2.104639	0.515494	0.001930	0.714899
-10.158368	-2.018035	0.520499	0.002021	0.714898
-10.159776	-2.016428	0.525504	0.002021	0.714901
-9.860617	-2.073007	0.530509	0.001965	0.714895
-9.877992	-2.087511	0.535514	0.001968	0.714860
-10.811474	-2.054994	0.540518	0.002142	0.714595
-10.788137	-2.058424	0.545523	0.002137	0.714597
-10.745103	-2.060292	0.550528	0.002129	0.714608
-10.960713	-2.025831	0.555533	0.002169	0.714601
-10.718887	-2.064963	0.560538	0.002124	0.714609
-10.946917	-2.026834	0.565542	0.002166	0.714604
-11.283621	-2.083410	0.570547	0.002229	0.714373
-11.951658	-2.015460	0.575552	0.002353	0.714271
-11.841765	-2.038240	0.580557	0.002333	0.714265
-11.794825	-2.043008	0.585562	0.002324	0.714273
-12.006195	-2.007020	0.590566	0.002363	0.714269
-11.642890	-2.070823	0.595571	0.002295	0.714272
-11.248587	-2.138969	0.600576	0.002222	0.714276
-12.613201	-2.046999	0.605581	0.002476	0.713976
-12.733852	-2.027997	0.610586	0.002498	0.713971
-12.767524	-2.026220	0.615590	0.002504	0.713963
-12.983503	-1.988232	0.620595	0.002544	0.713962
-12.847285	-2.009849	0.625600	0.002519	0.713967
-12.809110	-2.021541	0.630605	0.002512	0.713958
-12.619514	-2.053140	0.635610	0.002476	0.713963
-12.861134	-2.111467	0.640614	0.002521	0.713761
-13.797989	-2.004326	0.645619	0.002696	0.713643
-13.312989	-2.085967	0.650624	0.002605	0.713652
-13.743107	-2.013986	0.655629	0.002685	0.713643
-13.577093	-2.040993	0.660634	0.002654	0.713649
-13.518180	-2.052255	0.665638	0.002643	0.713647
-13.866349	-1.990792	0.670643	0.002708	0.713646
-13.968457	-2.067648	0.675648	0.002727	0.713457
-14.780368	-1.976577	0.680653	0.002878	0.713351
-14.531845	-2.016795	0.685658	0.002831	0.713359
-14.504201	-2.024840	0.690662	0.002826	0.713353
-14.337828	-2.053247	0.695667	0.002795	0.713356
-14.252675	-2.067104	0.700672	0.002779	0.713359
-14.908085	-1.954313	0.705677	0.002901	0.713351
-14.782756	-2.061018	0.710682	0.002878	0.713183
-15.603176	-1.997745	0.715686	0.003030	0.713019
-15.380574	-2.036525	0.720691	0.002989	0.713021
-15.715144	-1.974815	0.725696	0.003051	0.713025
-15.517054	-2.015738	0.730701	0.003014	0.713014
-15.238113	-2.060006	0.735706	0.002962	0.713025
-15.659516	-1.990276	0.740710	0.003040	0.713015
-15.693079	-1.998121	0.745715	0.003046	0.712987
-16.104363	-2.063747	0.750720	0.003123	0.712711
-16.574745	-1.985286	0.755725	0.003210	0.712700
-16.662069	-1.964336	0.760730	0.003227	0.712711
-16.311388	-2.029075	0.765734	0.003161	0.712707
-16.451463	-2.006292	0.770739	0.003187	0.712703
-16.646313	-1.969869	0.775744	0.003223	0.712707
-16.482494	-2.003978	0.780749	0.003193	0.712697
-16.600747	-2.082801	0.785754	0.003215	0.712498
-17.885204	-1.913950	0.790758	0.003454	0.712379
-17.395685	-2.001233	0.795763	0.003362	0.712379
-16.930041	-2.079559	0.800768	0.003276	0.712388
-17.838735	-1.923152	0.805773	0.003445	0.712378
-17.488410	-1.980656	0.810778	0.003379	0.712388
-17.096055	-2.054348	0.815782	0.003306	0.712380
-17.406326	-2.033642	0.820787	0.003364	0.712312
-18.389153	-1.970496	0.825792	0.003547	0.712089
-18.210027	-2.006703	0.830797	0.003513	0.712080
-17.997254	-2.040405	0.835802	0.003474	0.712089
-18.422766	-1.966328	0.840806	0.003553	0.712086
-18.550263	-1.943982	0.845811	0.003576	0.712085
-18.292463	-1.987784	0.850816	0.003528	0.712090
-18.457454	-1.963693	0.855821	0.003559	0.712079
-18.570306	-2.060419	0.860826	0.003580	0.711846
-19.390093	-1.960989	0.865830	0.003732	0.711754
-19.199144	-1.995465	0.870835	0.003697	0.711753
-19.000530	-2.028684	0.875840	0.003660	0.711758
-19.473905	-1.947485	0.880845	0.003748	0.711751
-18.772857	-2.067335	0.885850	0.003617	0.711762
-19.051384	-2.021952	0.890854	0.003669	0.711753
-19.554903	-2.039146	0.895859	0.003762	0.711540
-19.875886	-2.025916	0.900864	0.003822	0.711453
-20.044091	-2.000345	0.905869	0.003853	0.711444
-20.269537	-1.955692	0.910874	0.003895	0.711454
-19.848974	-2.032884	0.915878	0.003817	0.711449
-19.837694	-2.034601	0.920883	0.003815	0.711450
-19.886727	-2.022831	0.925888	0.003824	0.711456
-20.735342	-1.998079	0.930893	0.003982	0.711204
-21.104816	-1.965898	0.935898	0.004050	0.711137
-20.949094	-1.996718	0.940902	0.004021	0.711131
-21.351097	-1.925141	0.945907	0.004096	0.711131
-21.008537	-1.983467	0.950912	0.004032	0.711137
-20.725416	-2.038593	0.955917	0.003979	0.711128
-20.755026	-2.028486	0.960922	0.003985	0.711138
-20.793316	-2.076163	0.965926	0.003992	0.711029
-21.574087	-2.019867	0.970931	0.004137	0.710864
-21.403640	-2.045451	0.975936	0.004105	0.710874
-21.829698	-1.975255	0.980941	0.004184	0.710862
-21.473147	-2.034865	0.985946	0.004118	0.710870
-21.396955	-2.050104	0.990950	0.004104	0.710867
-21.731594	-1.995652	0.995955	0.004166	0.710857
-21.992051	-2.112017	1.000960	0.004214	0.710532
-22.303547	-2.060512	1.005965	0.004272	0.710525
-22.915306	-1.944206	1.010970	0.004386	0.710539
-22.656698	-1.997033	1.015974	0.004338	0.710526
-22.632337	-2.000026	1.020979	0.004333	0.710529
-22.750732	-1.976368	1.025984	0.004355	0.710534
-22.809869	-1.968937	1.030989	0.004366	0.710528
-22.986067	-2.086762	1.035994	0.004399	0.710230
-23.298973	-2.037347	1.040998	0.004457	0.710218
-23.963303	-1.920812	1.046003	0.004580	0.710214
-23.309081	-2.034453	1.051008	0.004458	0.710220
-23.427543	-2.017932	1.056013	0.004480	0.710211
-23.555374	-1.991304	1.061018	0.004504	0.710219
-23.641882	-1.978954	1.066022	0.004520	0.710213
-24.089716	-2.047441	1.071027	0.004603	0.709917
-24.437403	-1.996547	1.076032	0.004668	0.709895
-24.714480	-1.951834	1.081037	0.004719	0.709886
-24.272147	-2.026858	1.086042	0.004637	0.709894
-24.447192	-1.996854	1.091046	0.004669	0.709892
-24.838916	-1.928781	1.096051	0.004742	0.709888
-24.480412	-1.990545	1.101056	0.004675	0.709893
-24.640236	-2.028094	1.106061	0.004705	0.709761
-25.588063	-1.941038	1.111066	0.004881	0.709598
-25.453469	-1.967543	1.116070	0.004856	0.709593
-25.224444	-2.008535	1.121075	0.004813	0.709593
-25.023044	-2.040780	1.126080	0.004776	0.709600
-25.319561	-1.992990	1.131085	0.004831	0.709590
-25.450237	-1.965467	1.136090	0.004855	0.709599
-25.239715	-2.064424	1.141094	0.004816	0.709476
-26.557863	-1.936959	1.146099	0.005061	0.709261
-26.225522	-1.992816	1.151104	0.004999	0.709268
-26.243836	-1.993590	1.156109	0.005003	0.709260
-26.189701	-2.001035	1.161114	0.004992	0.709265
-26.332038	-1.978613	1.166118	0.005019	0.709259
-26.492358	-1.949983	1.171123	0.005049	0.709260
-25.901601	-2.075726	1.176128	0.004938	0.709219
-26.969899	-2.020193	1.181133	0.005137	0.708949
-26.950951	-2.019419	1.186138	0.005134	0.708958
-27.048445	-2.004714	1.191142	0.005152	0.708952
-27.244783	-1.970755	1.196147	0.005188	0.708951
-27.006050	-2.008724	1.201152	0.005144	0.708960
-26.999935	-2.015682	1.206157	0.005142	0.708948
-26.952041	-2.071213	1.211162	0.005133	0.708855
-27.971446	-1.999885	1.216166	0.005323	0.708634
-28.022598	-1.990866	1.221171	0.005332	0.708634
-27.733776	-2.038232	1.226176	0.005279	0.708642
-28.378402	-1.929207	1.231181	0.005398	0.708631
-27.972468	-1.998731	1.236186	0.005323	0.708636
-27.659678	-2.056448	1.241190	0.005265	0.708633
-27.964786	-2.047679	1.246195	0.005321	0.708542
-28.657997	-2.018892	1.251200	0.005450	0.708352
-28.511663	-2.050019	1.256205	0.005423	0.708342
-28.622773	-2.025094	1.261210	0.005443	0.708352
-28.635259	-2.025538	1.266214	0.005446	0.708347
-28.703116	-2.014360	1.271219	0.005458	0.708346
-28.445797	-2.058178	1.276224	0.005410	0.708350
-29.061536	-2.088574	1.281229	0.005525	0.708069
-29.649056	-2.011325	1.286234	0.005634	0.708014
-29.763247	-1.992160	1.291238	0.005655	0.708012
-29.766516	-1.993895	1.296243	0.005656	0.708008
-29.611071	-2.016833	1.301248	0.005627	0.708018
-29.597688	-2.024261	1.306253	0.005624	0.708008
-29.424374	-2.052096	1.311258	0.005592	0.708014
-30.011738	-2.084052	1.316262	0.005701	0.707740
-30.457600	-2.026551	1.321267	0.005784	0.707696
-30.152755	-2.078377	1.326272	0.005727	0.707701
-30.557987	-2.010644	1.331277	0.005802	0.707693
-30.518627	-2.014450	1.336282	0.005795	0.707699
-30.165339	-2.078413	1.341286	0.005729	0.707698
-30.256359	-2.112290	1.346291	0.005746	0.707597
-31.515216	-1.995337	1.351296	0.005980	0.707382
-31.201129	-2.056865	1.356301	0.005922	0.707371
-31.409579	-2.016736	1.361306	0.005960	0.707377
-31.699117	-1.966431	1.366310	0.006014	0.707375
-31.565150	-1.991341	1.371315	0.005989	0.707373
-31.325854	-2.031993	1.376320	0.005944	0.707377
-31.527385	-2.000214	1.381325	0.005982	0.707369
-31.848334	-2.076373	1.386330	0.006041	0.707101
-31.893409	-2.080139	1.391334	0.006050	0.707078
-32.211012	-2.025919	1.396339	0.006109	0.707073
-32.195776	-2.024729	1.401344	0.006106	0.707081
-32.289619	-2.010782	1.406349	0.006123	0.707076
-32.210106	-2.022409	1.411354	0.006108	0.707081
-32.463341	-1.990237	1.416358	0.006155	0.707055
-33.193728	-2.013829	1.421363	0.006291	0.706747
-32.818492	-2.077861	1.426368	0.006221	0.706753
-33.301640	-1.995995	1.431373	0.006311	0.706744
-33.254519	-2.000179	1.436378	0.006302	0.706753
-32.880943	-2.067840	1.441382	0.006233	0.706751
-33.140564	-2.023408	1.446387	0.006281	0.706748
-33.153097	-2.023565	1.451392	0.006283	0.706743
-33.951871	-2.033184	1.456397	0.006432	0.706438
-33.765406	-2.061899	1.461402	0.006397	0.706447
-33.961852	-2.029193	1.466406	0.006433	0.706443
-34.309118	-1.969409	1.471411	0.006498	0.706439
-34.039925	-2.014074	1.476416	0.006448	0.706446
-34.084610	-2.010402	1.481421	0.006456	0.706437
-34.232679	-1.979756	1.486426	0.006483	0.706446
-34.332361	-2.079096	1.491430	0.006502	0.706211
-35.276080	-1.954142	1.496435	0.006677	0.706124
-35.115282	-1.979488	1.501440	0.006647	0.706131
-35.018474	-2.001579	1.506445	0.006629	0.706121
-35.049374	-1.992753	1.511450	0.006635	0.706128
-34.899610	-2.021256	1.516454	0.006607	0.706125
-35.247680	-1.960006	1.521459	0.006672	0.706123
-34.802216	-2.085905	1.526464	0.006589	0.706030
-35.783421	-1.998615	1.531469	0.006771	0.705854
-35.964680	-1.962287	1.536474	0.006805	0.705862
-35.859183	-1.983055	1.541478	0.006785	0.705858
-35.667237	-2.019000	1.546483	0.006749	0.705855
-35.416691	-2.057008	1.551488	0.006703	0.705869
-35.976429	-1.964350	1.556493	0.006807	0.705855
-35.751176	-2.105994	1.561498	0.006765	0.705651
-36.419881	-2.051242	1.566502	0.006889	0.705521
-36.910178	-1.965798	1.571507	0.006980	0.705517
-36.638847	-2.010386	1.576512	0.006930	0.705525
-36.817527	-1.983209	1.581517	0.006963	0.705516
-36.710804	-1.998531	1.586522	0.006943	0.705524
-36.524543	-2.032648	1.591526	0.006908	0.705522
-37.055816	-2.051476	1.596531	0.007007	0.705294
-37.682688	-1.979137	1.601536	0.007123	0.705215
-37.943254	-1.938018	1.606541	0.007172	0.705204
-37.555806	-2.004900	1.611546	0.007100	0.705209
-37.899179	-1.944056	1.616550	0.007163	0.705208
-38.004848	-1.927797	1.621555	0.007183	0.705203
-37.571399	-2.000399	1.626560	0.007102	0.705213
-37.492383	-2.047072	1.631565	0.007087	0.705147
-38.313269	-2.031100	1.636570	0.007240	0.704885
-38.449118	-2.009615	1.641574	0.007265	0.704880
-38.531323	-1.996259	1.646579	0.007280	0.704877
-37.988577	-2.088931	1.651584	0.007179	0.704886
-38.534330	-1.995648	1.656589	0.007281	0.704878
-38.869117	-1.931683	1.661594	0.007343	0.704887
-38.205333	-2.103166	1.666598	0.007219	0.704780
-39.332219	-1.999333	1.671603	0.007429	0.704584
-39.373871	-1.988365	1.676608	0.007437	0.704592
-39.719020	-1.930959	1.681613	0.007501	0.704584
-39.250724	-2.012646	1.686618	0.007414	0.704588
-39.363501	-1.993414	1.691622	0.007434	0.704586
-39.465029	-1.976845	1.696627	0.007453	0.704583
-39.464730	-2.005388	1.701632	0.007453	0.704526
-40.502840	-1.955671	1.706637	0.007646	0.704253
-40.145635	-2.017672	1.711642	0.007580	0.704257
-40.296482	-1.990916	1.716646	0.007608	0.704257
-40.340312	-1.985407	1.721651	0.007616	0.704252
-40.241789	-1.999005	1.726656	0.007597	0.704260
-40.454249	-1.964167	1.731661	0.007637	0.704255
-40.270790	-1.994921	1.736666	0.007603	0.704259
-40.576828	-2.083174	1.741670	0.007659	0.703971
-41.050287	-2.011554	1.746675	0.007747	0.703945
-41.007555	-2.014356	1.751680	0.007739	0.703955
-41.205936	-1.982685	1.756685	0.007776	0.703948
-41.459169	-1.937054	1.761690	0.007823	0.703949
-40.959570	-2.026070	1.766694	0.007730	0.703949
-40.968552	-2.049062	1.771699	0.007732	0.703900
-42.164172	-1.965986	1.776704	0.007954	0.703638
-42.233213	-1.959073	1.781709	0.007967	0.703627
-42.275205	-1.949171	1.786714	0.007975	0.703632
-42.038570	-1.990260	1.791718	0.007931	0.703635
-42.235123	-1.959453	1.796723	0.007967	0.703626
-42.181825	-1.965611	1.801728	0.007957	0.703633
-42.169723	-1.971851	1.806733	0.007955	0.703625
-42.256398	-2.040962	1.811738	0.007971	0.703455
-42.911755	-1.980629	1.816742	0.008093	0.703341
-43.071248	-1.957123	1.821747	0.008122	0.703331
-42.732649	-2.012063	1.826752	0.008059	0.703342
-42.858446	-1.993908	1.831757	0.008082	0.703334
-42.781492	-2.005175	1.836762	0.008068	0.703339
-42.931343	-1.979212	1.841766	0.008096	0.703338
-43.418658	-2.020723	1.846771	0.008186	0.703079
-43.723551	-2.002284	1.851776	0.008243	0.703006
-43.936323	-1.969044	1.856781	0.008283	0.702997
-43.904059	-1.972306	1.861786	0.008276	0.703002
-43.831769	-1.985332	1.866790	0.008263	0.703002
-43.828095	-1.990181	1.871795	0.008262	0.702994
-43.628263	-2.021427	1.876800	0.008225	0.703003
-44.057395	-2.060961	1.881805	0.008305	0.702769
-45.043635	-1.924302	1.886810	0.008488	0.702690
-44.803332	-1.965586	1.891814	0.008443	0.702693
-44.608852	-2.005073	1.896819	0.008407	0.702683
-44.549413	-2.011173	1.901824	0.008396	0.702693
-44.612378	-2.002942	1.906829	0.008407	0.702687
-44.437960	-2.033869	1.911834	0.008375	0.702687
-44.857118	-2.085204	1.916838	0.008453	0.702433
-45.503894	-2.004610	1.921843	0.008573	0.702363
-45.516040	-1.998141	1.926848	0.008575	0.702372
-45.385041	-2.024802	1.931853	0.008551	0.702365
-45.514681	-1.999507	1.936858	0.008575	0.702370
-45.779678	-1.953590	1.941862	0.008624	0.702367
-45.718886	-1.967423	1.946867	0.008613	0.702362
-45.921915	-2.053450	1.951872	0.008650	0.702115
-46.478199	-1.978245	1.956877	0.008754	0.702066
-46.858246	-1.908030	1.961882	0.008824	0.702071
-46.286874	-2.009006	1.966886	0.008718	0.702073
-46.441999	-1.984532	1.971891	0.008747	0.702067
-46.542002	-1.963016	1.976896	0.008765	0.702075
-46.494626	-1.976386	1.981901	0.008756	0.702065
-46.741149	-2.044843	1.986906	0.008802	0.701838
-47.576387	-1.943376	1.991910	0.008958	0.701742
-47.674067	-1.926789	1.996915	0.008976	0.701741
-47.345002	-1.984327	2.001920	0.008914	0.701743

-47.412916	-1.972761	2.011917	0.008927	0.701742
-47.368750	-1.981142	2.021914	0.008918	0.701742
-47.300885	-2.058586	2.031910	0.008905	0.701610
-48.467302	-1.938971	2.041907	0.009122	0.701431
-47.861593	-2.023627	2.051904	0.009009	0.701479
-47.630956	-1.967032	2.061901	0.008966	0.701677
-47.385186	-2.022869	2.071898	0.008920	0.701653
-47.334431	-1.996935	2.081894	0.008911	0.701725
-47.200571	-2.012079	2.091891	0.008886	0.701743
-47.123548	-2.025739	2.101888	0.008871	0.701743
-47.239231	-2.005694	2.111885	0.008892	0.701742
-47.096903	-2.031617	2.121882	0.008866	0.701742
-47.279639	-1.999924	2.131878	0.008899	0.701740
-47.343756	-1.987412	2.141875	0.008911	0.701743
-47.143190	-2.017154	2.151872	0.008874	0.701755
-46.601291	-1.957099	2.161869	0.008773	0.702073
-46.165352	-2.035530	2.171866	0.008691	0.702072
-46.293049	-2.014734	2.181862	0.008715	0.702068
-46.222715	-2.026273	2.191859	0.008701	0.702071
-46.169710	-1.972623	2.201856	0.008691	0.702199
-45.344048	-2.035973	2.211853	0.008537	0.702369
-45.229839	-2.056998	2.221850	0.008516	0.702368
-45.493941	-2.010721	2.231846	0.008565	0.702366
-45.454772	-1.979010	2.241843	0.008557	0.702445
-44.594234	-2.010762	2.251840	0.008397	0.702691
-44.659640	-1.998329	2.261837	0.008409	0.702693
-44.573315	-2.014575	2.271834	0.008393	0.702692
-44.187065	-1.990187	2.281830	0.008321	0.702881
-43.609110	-2.032340	2.291827	0.008213	0.703004
-43.833267	-1.992105	2.301824	0.008254	0.703005
-43.845776	-1.988949	2.311821	0.008256	0.703007
-42.802849	-2.018543	2.321818	0.008062	0.703323
-43.018371	-1.973035	2.331814	0.008102	0.703338
-42.814154	-2.008790	2.341811	0.008064	0.703340
-42.831967	-1.962837	2.351808	0.008067	0.703427
-42.084516	-1.994338	2.361805	0.007927	0.703632
-41.991154	-2.011606	2.371802	0.007910	0.703632
-42.128126	-1.987033	2.381798	0.007935	0.703632
-41.321841	-1.990247	2.391795	0.007785	0.703916
-41.102881	-2.011231	2.401792	0.007744	0.703953
-40.937382	-2.039422	2.411789	0.007713	0.703956
-40.944110	-2.014975	2.421786	0.007714	0.704003
-40.376402	-1.989529	2.431782	0.007608	0.704259
-40.064401	-2.046823	2.441779	0.007550	0.704256
-40.480175	-1.971846	2.451776	0.007627	0.704258
-39.790866	-1.974623	2.461773	0.007498	0.704501
-39.481053	-1.986849	2.471770	0.007440	0.704588
-39.588848	-1.968060	2.481766	0.007460	0.704587
-39.092807	-2.005219	2.491763	0.007368	0.704691
-38.369824	-2.038518	2.501760	0.007233	0.704884
-38.442239	-2.026115	2.511757	0.007246	0.704883
-38.609426	-1.996272	2.521754	0.007277	0.704884
-38.107747	-1.954225	2.531750	0.007183	0.705149
-37.920463	-1.957879	2.541747	0.007148	0.705209
-37.782244	-1.982833	2.551744	0.007122	0.705209
-37.402436	-1.967418	2.561741	0.007051	0.705377
-36.906419	-1.984506	2.571738	0.006959	0.705521
-36.873525	-1.990411	2.581734	0.006953	0.705521
-36.795250	-1.980208	2.591731	0.006938	0.705570
-35.951551	-1.984732	2.601728	0.006781	0.705864
-35.767967	-2.018859	2.611725	0.006746	0.705861
-35.967073	-1.983911	2.621722	0.006783	0.705861
-35.727298	-1.961019	2.631718	0.006738	0.705993
-35.046174	-2.019548	2.641715	0.006611	0.706120
-35.353037	-1.962438	2.651712	0.006668	0.706125
-34.979455	-1.999567	2.661709	0.006598	0.706185
-34.729999	-1.917080	2.671706	0.006552	0.706440
-34.255605	-2.002968	2.681702	0.006463	0.706438
-34.481979	-1.962462	2.691699	0.006505	0.706439
-33.466863	-1.991390	2.701696	0.006316	0.706745
-33.301811	-2.019568	2.711693	0.006285	0.706747
-33.388681	-2.003190	2.721690	0.006301	0.706750
-33.290310	-1.965782	2.731686	0.006282	0.706860
-32.569963	-1.988707	2.741683	0.006148	0.707073
-32.533630	-1.993667	2.751680	0.006141	0.707076
-32.402847	-2.016980	2.761677	0.006116	0.707076
-32.047187	-1.946788	2.771674	0.006050	0.707345
-31.645183	-2.005515	2.781670	0.005975	0.707371
-31.882948	-1.963992	2.791667	0.006019	0.707370
-31.361158	-1.965311	2.801664	0.005922	0.707554
-30.782639	-1.996976	2.811661	0.005814	0.707698
-30.765615	-2.002155	2.821658	0.005810	0.707694
-30.565806	-2.039407	2.831654	0.005773	0.707691
-30.275859	-1.938666	2.841651	0.005719	0.707997
-29.914071	-1.996837	2.851648	0.005651	0.708010
-29.889222	-2.002319	2.861645	0.005646	0.708009
-29.636399	-1.951356	2.871642	0.005599	0.708201
-28.862151	-2.016937	2.881638	0.005455	0.708347
-29.307955	-1.937754	2.891635	0.005538	0.708347
-28.756780	-2.035954	2.901632	0.005435	0.708347
-28.290281	-1.976830	2.911629	0.005348	0.708633
-28.158116	-1.999607	2.921626	0.005323	0.708635
-28.181489	-1.995364	2.931622	0.005327	0.708635
-28.080133	-1.930272	2.941619	0.005308	0.708802
-27.301925	-1.993365	2.951616	0.005163	0.708954
-27.374996	-1.979523	2.961613	0.005176	0.708956
-27.260597	-1.982190	2.971610	0.005155	0.708992
-26.450598	-1.991724	2.981606	0.005004	0.709262
-26.507495	-1.985529	2.991603	0.005014	0.709255
-26.200286	-2.039812	3.001600	0.004957	0.709256
-26.172002	-1.946619	3.011597	0.004951	0.709453
-25.718484	-1.957120	3.021594	0.004867	0.709594
-25.637714	-1.972297	3.031590	0.004851	0.709593
-25.726211	-1.919287	3.041587	0.004868	0.709668
-24.776642	-1.979980	3.051584	0.004691	0.709885
-24.880055	-1.960808	3.061581	0.004710	0.709887
-24.886998	-1.959142	3.071578	0.004711	0.709888
-24.240683	-1.920742	3.081574	0.004590	0.710195
-23.975075	-1.961428	3.091571	0.004540	0.710209
-23.600740	-2.026653	3.101568	0.004471	0.710212
-23.672853	-1.937883	3.111565	0.004484	0.710365
-22.787996	-2.013218	3.121562	0.004319	0.710529
-23.009553	-1.976670	3.131558	0.004360	0.710524
-22.997571	-1.978297	3.141555	0.004357	0.710525
-22.133404	-1.980722	3.151552	0.004196	0.710828
-22.233595	-1.941612	3.161549	0.004215	0.710871
-21.880838	-2.005883	3.171546	0.004149	0.710869
-22.297727	-1.888764	3.181542	0.004226	0.710955
-21.334242	-1.973177	3.191539	0.004047	0.711129
-21.452635	-1.951571	3.201536	0.004069	0.711131
-21.658585	-1.891177	3.211533	0.004107	0.711178
-20.786465	-1.912460	3.221530	0.003944	0.711446
-20.537923	-1.957219	3.231526	0.003898	0.711446
-20.466567	-1.970209	3.241523	0.003884	0.711446
-19.920113	-1.930386	3.251520	0.003782	0.711720
-19.727973	-1.946436	3.261517	0.003746	0.711756
-19.473834	-1.990938	3.271514	0.003699	0.711758
-19.531409	-1.908311	3.281510	0.003709	0.711903
-18.406809	-2.018004	3.291507	0.003500	0.712084
-18.856990	-1.937003	3.301504	0.003583	0.712086
-18.752754	-1.956086	3.311501	0.003564	0.712085
-18.067879	-1.944325	3.321498	0.003436	0.712352
-18.013759	-1.938942	3.331494	0.003426	0.712383
-17.983687	-1.944888	3.341491	0.003420	0.712382
-17.694974	-1.913027	3.351488	0.003366	0.712548
-17.103281	-1.938663	3.361485	0.003255	0.712708
-16.993536	-1.958021	3.371482	0.003235	0.712708
-17.285202	-1.881165	3.381478	0.003289	0.712758
-15.987355	-1.981114	3.391475	0.003047	0.713020
-15.982842	-1.979758	3.401472	0.003046	0.713025
-16.160347	-1.948327	3.411469	0.003079	0.713025
-15.801047	-1.919455	3.421466	0.003012	0.713210
-15.252166	-1.942174	3.431462	0.002909	0.713360
-15.092879	-1.970514	3.441459	0.002879	0.713360
-15.259032	-1.940989	3.451456	0.002910	0.713360
-14.526956	-1.929199	3.461453	0.002774	0.713644
-14.310298	-1.962415	3.471450	0.002733	0.713655
-14.418866	-1.944840	3.481446	0.002753	0.713651
-14.094585	-1.932523	3.491443	0.002692	0.713791
-13.578441	-1.935695	3.501440	0.002596	0.713968
-13.589969	-1.932657	3.511437	0.002598	0.713970
-13.570618	-1.924031	3.521434	0.002594	0.713995
-12.714651	-1.936103	3.531430	0.002435	0.714274
-12.549433	-1.965695	3.541427	0.002404	0.714274
-12.597915	-1.956191	3.551424	0.002413	0.714276
-12.342772	-1.921651	3.561421	0.002365	0.714436
-11.738448	-1.941704	3.571418	0.002252	0.714610
-11.883096	-1.916800	3.581414	0.002279	0.714609
-11.653376	-1.952686	3.591411	0.002236	0.714619
-11.159185	-1.895249	3.601408	0.002144	0.714908
-10.791439	-1.960250	3.611405	0.002075	0.714910
-10.965103	-1.929350	3.621402	0.002107	0.714910
-10.568872	-1.898520	3.631398	0.002033	0.715112
-10.141316	-1.914373	3.641395	0.001953	0.715232
-10.068530	-1.926275	3.651392	0.001940	0.715234
-9.765477	-1.950711	3.661389	0.001883	0.715293
-9.190062	-1.924229	3.671386	0.001776	0.715549
-9.109832	-1.940531	3.681382	0.001760	0.715546
-9.129231	-1.937271	3.691379	0.001764	0.715546
-9.062692	-1.840514	3.701376	0.001751	0.715761
-7.864960	-1.991730	3.711373	0.001528	0.715885
-7.927330	-1.980539	3.721370	0.001539	0.715885
-7.449116	-2.066791	3.731366	0.001450	0.715884
-7.439617	-1.994215	3.741363	0.001448	0.716031
-6.919176	-2.035640	3.751360	0.001351	0.716133
-6.739353	-2.066606	3.761357	0.001317	0.716136
-7.051436	-2.011841	3.771354	0.001375	0.716135
-6.596784	-2.001763	3.781350	0.001290	0.716315
-6.127992	-2.017546	3.791347	0.001203	0.716450
-6.178053	-2.008193	3.801344	0.001212	0.716451
-5.950358	-2.048159	3.811341	0.001170	0.716453
-5.684333	-1.965586	3.821338	0.001120	0.716710
-5.301800	-2.010626	3.831334	0.001048	0.716756
-5.218169	-2.025126	3.841331	0.001033	0.716758
-5.075814	-2.004832	3.851328	0.001006	0.716848
-4.142051	-2.051395	3.861325	0.000832	0.717086
-4.306717	-2.024235	3.871322	0.000862	0.717082
-4.033473	-2.072747	3.881318	0.000811	0.717082
-4.242707	-1.954281	3.891315	0.000850	0.717243
-3.271275	-2.058351	3.901312	0.000669	0.717380
-3.375902	-2.038330	3.911309	0.000688	0.717383
-3.072690	-2.090479	3.921306	0.000631	0.717387
-2.881936	-1.996056	3.931302	0.000596	0.717642
-2.420123	-2.047351	3.941299	0.000510	0.717703
-2.321840	-2.063155	3.951296	0.000491	0.717707
-2.305304	-2.047355	3.961293	0.000488	0.717744
-1.901749	-1.980403	3.971290	0.000412	0.718019
-1.828892	-1.993497	3.981286	0.000399	0.718019
-1.992750	-1.966328	3.991283	0.000429	0.718016
-1.613743	-1.877060	4.001280	0.000358	0.718326
-1.334207	-1.910144	4.011277	0.000306	0.718359
-1.388287	-1.892198	4.021274	0.000316	0.718376
-1.187774	-1.790421	4.031270	0.000278	0.718648
-1.031031	-1.821384	4.041267	0.000249	0.718642
-0.977311	-1.749058	4.051264	0.000238	0.718804
-0.985649	-1.666730	4.061261	0.000240	0.718964
-1.159981	-1.578394	4.071258	0.000272	0.719077
-0.900117	-1.525691	4.081254	0.000223	0.719273
-0.974155	-1.440052	4.091251	0.000237	0.719416
-0.836611	-1.370552	4.101248	0.000211	0.719602
-0.698759	-1.294499	4.111245	0.000185	0.719800
-0.438974	-1.289478	4.121242	0.000136	0.719902
-0.585412	-1.109622	4.131238	0.000163	0.720205
-0.574194	-1.040144	4.141235	0.000161	0.720346
-0.432467	-0.966183	4.151232	0.000134	0.720542
-0.209335	-0.851090	4.161229	0.000093	0.720847
-0.201065	-0.779989	4.171226	0.000091	0.720990
-0.314247	-0.675763	4.181222	0.000112	0.721156
-0.348501	-0.525874	4.191219	0.000118	0.721439
-0.182106	-0.425614	4.201216	0.000086	0.721695
-0.243174	-0.287430	4.211213	0.000098	0.721945
-0.260500	-0.147162	4.221210	0.000100	0.722215
-0.026110	-0.057235	4.231206	0.000057	0.722474
-0.155497	0.115910	4.241203	0.000080	0.722769
0.000000	0.281311	4.251200	0.000051	0.723148

-0.042819	0.911214	4.256205	0.000059	0.724368
0.330844	2.107702	4.261210	-0.000012	0.726837
0.414503	3.948490	4.266214	-0.000029	0.730450
0.476116	6.343192	4.271219	-0.000042	0.735106
0.731642	9.215382	4.276224	-0.000092	0.740714
1.229287	12.523218	4.281229	-0.000186	0.747190
1.826267	16.275574	4.286234	-0.000300	0.754478
1.950434	20.510175	4.291238	-0.000326	0.762438
2.583708	25.060426	4.296243	-0.000447	0.771063
3.003132	30.017760	4.301248	-0.000529	0.780264
3.431077	35.321390	4.306253	-0.000612	0.789981
3.922916	40.935609	4.311258	-0.000707	0.800151
4.394123	46.853107	4.316262	-0.000799	0.810718
4.780341	53.066177	4.321267	-0.000875	0.821633
5.262468	59.539834	4.326272	-0.000969	0.832877
5.674762	66.232255	4.331277	-0.001050	0.844318
8.076677	72.825676	4.336282	-0.001502	0.856023
9.212176	79.868754	4.341286	-0.001718	0.867938
9.708430	87.212779	4.346291	-0.001815	0.879996
10.562962	94.670363	4.351296	-0.001979	0.892171
11.269207	102.313598	4.356301	-0.002116	0.904432
12.691897	110.005570	4.361306	-0.002386	0.916798
13.487955	117.906350	4.366310	-0.002539	0.929150
14.442084	125.906212	4.371315	-0.002722	0.941530
15.264205	134.035689	4.376320	-0.002881	0.953907
16.074551	142.228433	4.381325	-0.003037	0.966215
16.884051	150.525280	4.386330	-0.003193	0.978519
17.210772	158.980207	4.391334	-0.003260	0.990774
18.250648	167.348876	4.396339	-0.003459	1.002934
19.579078	175.727939	4.401344	-0.003712	1.015032
20.222160	184.251134	4.406349	-0.003837	1.027021
21.092392	192.797623	4.411354	-0.004005	1.038957
22.100876	201.332014	4.416358	-0.004199	1.050773
22.874319	209.938106	4.421363	-0.004348	1.062498
23.602789	218.591920	4.426368	-0.004490	1.074148
24.337518	227.215475	4.431373	-0.004632	1.085634
25.342175	235.829869	4.436378	-0.004825	1.097047
26.120063	244.479618	4.441382	-0.004976	1.108338
26.528891	253.186654	4.446387	-0.005057	1.119507
27.320461	261.843162	4.451392	-0.005211	1.130584
27.892078	270.510009	4.456397	-0.005323	1.141520
28.751289	279.166424	4.461402	-0.005488	1.152399
29.540983	287.774995	4.466406	-0.005641	1.163103
30.087968	296.426634	4.471411	-0.005749	1.173711
30.634754	305.061557	4.476416	-0.005856	1.184203
30.929037	313.726236	4.481421	-0.005917	1.194588
31.928140	322.250792	4.486426	-0.006109	1.204859
32.567060	330.838355	4.491430	-0.006233	1.215044
33.134000	339.419655	4.496435	-0.006345	1.225124
34.221055	347.938325	4.501440	-0.006553	1.235150
34.884164	356.459188	4.506445	-0.006682	1.245016
35.311428	365.047648	4.511450	-0.006767	1.254835
35.810647	373.573078	4.516454	-0.006866	1.264520
36.540560	382.072956	4.521459	-0.007007	1.274147
37.156121	390.567946	4.526464	-0.007127	1.283674
37.773219	399.048652	4.531469	-0.007248	1.293116
38.155660	407.562600	4.536474	-0.007325	1.302482
38.487009	416.144748	4.541478	-0.007392	1.311845
39.161925	424.597707	4.546483	-0.007523	1.321065
39.926900	432.991384	4.551488	-0.007671	1.330174
40.590693	441.380455	4.556493	-0.007801	1.339198
41.065101	449.804034	4.561498	-0.007895	1.348164
41.671178	458.192618	4.566502	-0.008013	1.357057
42.440048	466.518354	4.571507	-0.008162	1.365855
43.048370	474.912894	4.576512	-0.008281	1.374640
43.464614	483.292885	4.581517	-0.008364	1.383320
44.024581	491.681527	4.586522	-0.008473	1.391980
44.466572	500.043677	4.591526	-0.008561	1.400539
45.164225	508.354527	4.596531	-0.008697	1.409037
45.876287	516.687869	4.601536	-0.008835	1.417509
46.427952	525.001729	4.606541	-0.008943	1.425885
46.879519	533.373957	4.611546	-0.009033	1.434252
47.629126	541.640980	4.616550	-0.009178	1.442516
47.925637	549.994816	4.621555	-0.009239	1.450744
48.159833	558.363256	4.626560	-0.009288	1.458930
48.719929	566.631831	4.631565	-0.009397	1.467026
49.315348	574.980455	4.636570	-0.009514	1.475159
49.980271	583.219994	4.641574	-0.009643	1.483154
50.363175	591.510816	4.646579	-0.009720	1.491111
50.897753	599.791653	4.651584	-0.009825	1.499040
51.453350	608.035779	4.656589	-0.009934	1.506895
51.931232	616.331696	4.661594	-0.010028	1.514746
52.386322	624.583260	4.666598	-0.010119	1.522511
52.593206	632.879833	4.671603	-0.010163	1.530242
53.234982	641.126036	4.676608	-0.010288	1.537951
53.677576	649.352070	4.681613	-0.010376	1.545575
54.243836	657.617607	4.686618	-0.010486	1.553214
54.775927	665.830004	4.691622	-0.010591	1.560763
55.115286	674.074941	4.696627	-0.010660	1.568277
55.758918	682.296020	4.701632	-0.010785	1.575778
56.135919	690.522064	4.706637	-0.010861	1.583208
56.533164	698.762083	4.711642	-0.010940	1.590620
57.129458	706.966603	4.716646	-0.011057	1.597993
57.605324	715.169472	4.721651	-0.011151	1.605314
58.164659	723.401978	4.726656	-0.011260	1.612639
58.325042	731.648486	4.731661	-0.011296	1.619888
58.943379	739.842584	4.736666	-0.011416	1.627122
59.438858	748.097669	4.741670	-0.011514	1.634360
59.993282	756.254068	4.746675	-0.011623	1.641488
60.662937	764.418405	4.751680	-0.011753	1.648608
60.863454	772.653347	4.756685	-0.011795	1.655694
61.282808	780.846521	4.761690	-0.011879	1.662744
61.400765	789.078467	4.766694	-0.011906	1.669756
61.877975	797.250144	4.771699	-0.012001	1.676736
62.385378	805.419907	4.776704	-0.012101	1.683689
62.509965	813.634635	4.781709	-0.012129	1.690600
63.149565	821.793183	4.786714	-0.012254	1.697504
63.395539	829.988020	4.791718	-0.012305	1.704359
63.895770	838.169100	4.796723	-0.012404	1.711208
64.613878	846.317027	4.801728	-0.012543	1.718030
65.006991	854.466112	4.806733	-0.012621	1.724784
65.183426	862.689806	4.811738	-0.012660	1.731545
65.634418	870.846280	4.816742	-0.012749	1.738259
65.799484	879.022811	4.821747	-0.012785	1.744928
66.259710	887.196444	4.826752	-0.012876	1.751606
66.573493	895.346136	4.831757	-0.012940	1.758221
67.253959	903.453320	4.836762	-0.013072	1.764823
67.581686	911.628950	4.841766	-0.013139	1.771410
67.959046	919.787856	4.846771	-0.013214	1.777966
68.430330	927.927270	4.851776	-0.013308	1.784494
68.809026	936.116289	4.856781	-0.013383	1.791026
69.181656	944.303447	4.861786	-0.013458	1.797532
69.396815	952.443996	4.866790	-0.013504	1.803958
69.826238	960.567309	4.871795	-0.013589	1.810374
70.271157	968.709275	4.876800	-0.013677	1.816784
70.481119	976.852555	4.881805	-0.013722	1.823144
71.107703	984.968400	4.886810	-0.013844	1.829510
71.441438	993.117693	4.891814	-0.013911	1.835845
71.559692	1001.281455	4.896819	-0.013939	1.842144
72.061833	1009.405227	4.901824	-0.014038	1.848435
72.698476	1017.506908	4.906829	-0.014162	1.854704
73.025150	1025.652241	4.911834	-0.014228	1.860949
73.148573	1033.821531	4.916838	-0.014256	1.867167
74.220631	1041.880218	4.921843	-0.014461	1.873391
74.809206	1049.992940	4.926848	-0.014576	1.879579
75.161433	1058.118820	4.931853	-0.014647	1.885729
75.604504	1066.274451	4.936858	-0.014735	1.891892
75.802077	1074.437444	4.941862	-0.014777	1.898012
76.033638	1082.571648	4.946867	-0.014826	1.904095
76.575598	1090.682979	4.951872	-0.014932	1.910176
77.064401	1098.798272	4.956877	-0.015029	1.916235
77.615371	1106.901059	4.961882	-0.015137	1.922272
77.661156	1115.077541	4.966886	-0.015151	1.928289
78.040726	1123.198192	4.971891	-0.015227	1.934282
78.609948	1131.301513	4.976896	-0.015338	1.940265
79.141515	1139.380642	4.981901	-0.015442	1.946208
79.360010	1147.580369	4.986906	-0.015489	1.952186
79.727114	1155.690525	4.991910	-0.015562	1.958097
80.352742	1163.738958	4.996915	-0.015684	1.963974
80.790683	1171.851836	5.001920	-0.015771	1.969859
81.050930	1179.975362	5.006925	-0.015825	1.975715
81.476530	1188.083064	5.011930	-0.015910	1.981560
81.580342	1196.230111	5.016934	-0.015934	1.987381
81.796135	1204.363400	5.021939	-0.015980	1.993188
82.391685	1212.442612	5.026944	-0.016096	1.998979
82.415245	1220.559830	5.031949	-0.016106	2.004720
82.756646	1228.670584	5.036954	-0.016175	2.010473
83.220345	1236.761656	5.041958	-0.016267	2.016209
83.878458	1244.812438	5.046963	-0.016394	2.021920
84.164252	1252.953312	5.051968	-0.016453	2.027640
84.608860	1261.073845	5.056973	-0.016541	2.033345
85.143634	1269.148075	5.061978	-0.016646	2.039012
85.621423	1277.214343	5.066982	-0.016741	2.044651
85.728041	1285.351181	5.071987	-0.016766	2.050286
86.311179	1293.440009	5.076992	-0.016880	2.055920
86.449676	1301.555855	5.081997	-0.016911	2.061513
86.820871	1309.662829	5.087002	-0.016985	2.067107
86.987263	1317.789728	5.092006	-0.017022	2.072680
87.304008	1325.890374	5.097011	-0.017086	2.078235
87.705229	1333.968483	5.102016	-0.017166	2.083767
87.982324	1342.048176	5.107021	-0.017223	2.089274
88.641017	1350.129621	5.112026	-0.017351	2.094805
88.893193	1358.238588	5.117030	-0.017404	2.100300
89.092467	1366.334615	5.122035	-0.017446	2.105767
89.634243	1374.461270	5.127040	-0.017552	2.111273
89.806872	1382.598881	5.132045	-0.017590	2.116737
90.056062	1390.674053	5.137050	-0.017642	2.122152
90.419917	1398.731721	5.142054	-0.017715	2.127552
90.915372	1406.801120	5.147059	-0.017812	2.132960
91.159798	1414.910443	5.152064	-0.017863	2.138356
91.202122	1423.009118	5.157069	-0.017877	2.143712
91.680839	1431.075573	5.162074	-0.017971	2.149074
92.075751	1439.175010	5.167078	-0.018050	2.154437
92.200592	1447.242003	5.172083	-0.018079	2.159740
92.668092	1455.324741	5.177088	-0.018171	2.165073
92.896000	1463.395077	5.182093	-0.018219	2.170361
93.283019	1471.496264	5.187098	-0.018296	2.175672
93.512882	1479.580428	5.192102	-0.018344	2.180944
93.750291	1487.660835	5.197107	-0.018394	2.186201
94.369729	1495.737736	5.202112	-0.018515	2.191479
94.757012	1503.810447	5.207117	-0.018592	2.196719
95.160278	1511.880799	5.212122	-0.018673	2.201947
95.397648	1519.960670	5.217126	-0.018722	2.207154
95.728637	1528.041011	5.222131	-0.018789	2.212357
96.175417	1536.130463	5.227136	-0.018878	2.217564
96.432357	1544.206818	5.232141	-0.018931	2.222734
96.857326	1552.281561	5.237146	-0.019015	2.227905
96.993528	1560.411142	5.242150	-0.019046	2.233073
97.449745	1568.459844	5.247155	-0.019136	2.238207
97.766269	1576.531772	5.252160	-0.019201	2.243331
97.916614	1584.624974	5.257165	-0.019234	2.248442
98.276993	1592.714180	5.262170	-0.019307	2.253557
98.515727	1600.786361	5.267174	-0.019356	2.258639
98.712122	1608.851810	5.272179	-0.019398	2.263702
99.058036	1616.943777	5.277184	-0.019468	2.268783
99.325343	1625.098901	5.282189	-0.019523	2.273886
99.499072	1633.157981	5.287194	-0.019561	2.278909
99.936166	1641.179961	5.292198	-0.019648	2.283920
100.230410	1649.225175	5.297203	-0.019708	2.288923
100.578439	1657.324850	5.302208	-0.019778	2.293952
100.811832	1665.365970	5.307213	-0.019827	2.298925
101.179284	1673.425339	5.312218	-0.019901	2.303910
101.406079	1681.508462	5.317222	-0.019948	2.308886
101.656747	1689.593413	5.322227	-0.020000	2.313855
102.143534	1697.641131	5.327232	-0.020096	2.318810
102.357580	1705.704660	5.332237	-0.020142	2.323741
102.961688	1713.739502	5.337242	-0.020259	2.328677
103.265693	1721.842194	5.342246	-0.020321	2.333619
103.536112	1729.900000	5.347251	-0.020377	2.338520
103.879124	1737.977209	5.352256	-0.020446	2.343428
103.858152	1746.079719	5.357261	-0.020448	2.348312
104.432537	1754.152286	5.362266	-0.020560	2.353216
104.585912	1762.240948	5.367270	-0.020594	2.358085
104.930622	1770.240823	5.372275	-0.020663	2.362906
105.171452	1778.335301	5.377280	-0.020714	2.367766
105.471342	1786.386262	5.382285	-0.020775	2.372594
105.924115	1794.451138	5.387290	-0.020865	2.377433
106.022642	1802.534795	5.392294	-0.020888	2.382245
106.204983	1810.592031	5.397299	-0.020928	2.387038
106.755373	1818.654641	5.402304	-0.021035	2.391854
106.957634	1826.720857	5.407309	-0.021078	2.396635
107.388568	1834.764078	5.412314	-0.021164	2.401410
107.669731	1842.828678	5.417318	-0.021222	2.406177
107.924330	1850.892774	5.422323	-0.021274	2.410932
108.330630	1858.975489	5.427328	-0.021356	2.415700
108.619223	1867.011244	5.432333	-0.021415	2.420422
108.916778	1875.085261	5.437338	-0.021475	2.425158
109.154194	1883.180534	5.442342	-0.021525	2.429893
109.501392	1891.300381	5.447347	-0.021595	2.434640
109.768703	1899.340217	5.452352	-0.021650	2.439326
109.848800	1907.384184	5.457357	-0.021670	2.443992
110.294535	1915.409318	5.462362	-0.021759	2.448665
110.790472	1923.462449	5.467366	-0.021856	2.453348
110.914882	1931.533038	5.472371	-0.021885	2.458005
111.105482	1939.607372	5.477376	-0.021926	2.462661
111.456963	1947.641239	5.482381	-0.021997	2.467296
112.109753	1955.671067	5.487386	-0.022123	2.471942
112.358717	1963.758090	5.492390	-0.022175	2.476583
112.878795	1971.766576	5.497395	-0.022277	2.481190
113.156905	1979.849971	5.502400	-0.022334	2.485813
113.267057	1987.937386	5.507405	-0.022360	2.490417
113.630603	1996.012277	5.512410	-0.022433	2.495025
114.069889	2004.042322	5.517414	-0.022521	2.499603
114.457155	2012.080545	5.522419	-0.022598	2.504175
114.769637	2020.163842	5.527424	-0.022662	2.508757
114.988824	2028.281899	5.532429	-0.022708	2.513345
115.235085	2036.333068	5.537434	-0.022759	2.517888
115.348233	2044.391232	5.542438	-0.022785	2.522417
115.774972	2052.390596	5.547443	-0.022870	2.526928
116.448305	2060.430563	5.552448	-0.023001	2.531471
116.579206	2068.476831	5.557453	-0.023031	2.535970
117.040903	2076.522230	5.562458	-0.023122	2.540484
117.461579	2084.558235	5.567462	-0.023206	2.544983
117.627989	2092.650334	5.572467	-0.023242	2.549486
117.999796	2100.730223	5.577472	-0.023317	2.553989
118.135172	2108.766436	5.582477	-0.023347	2.558443
118.451947	2116.813605	5.587482	-0.023411	2.562908
118.642380	2124.894372	5.592486	-0.023452	2.567376
118.801163	2132.968628	5.597491	-0.023487	2.571829
119.366379	2141.018603	5.602496	-0.023598	2.576290
119.558683	2149.058820	5.607501	-0.023639	2.580711
119.707025	2157.099633	5.612506	-0.023672	2.585123
119.843677	2165.190628	5.617510	-0.023703	2.589553
120.028936	2173.428403	5.622515	-0.023743	2.594059
120.417070	2181.428325	5.627520	-0.023820	2.598442
120.771601	2189.391870	5.632525	-0.023892	2.602795
121.291448	2197.391557	5.637530	-0.023994	2.607172
121.439200	2205.458494	5.642534	-0.024027	2.611552
121.633092	2213.505613	5.647539	-0.024068	2.615918
121.958964	2221.543283	5.652544	-0.024134	2.620280
122.038559	2229.554609	5.657549	-0.024154	2.624604
122.438083	2237.593948	5.662554	-0.024234	2.628957
122.702870	2245.681224	5.667558	-0.024289	2.633319
122.678088	2253.738528	5.672563	-0.024289	2.637640
123.322411	2261.735780	5.677568	-0.024415	2.641965
123.882791	2269.730536	5.682573	-0.024524	2.646276
124.414464	2277.779656	5.687578	-0.024629	2.650607
124.652541	2285.878498	5.692582	-0.024678	2.654938
124.632456	2293.933581	5.697587	-0.024680	2.659222
124.937287	2301.994947	5.702592	-0.024742	2.663523
125.006920	2310.056941	5.707597	-0.024760	2.667803
125.234568	2318.137497	5.712602	-0.024808	2.672096
125.593963	2326.201005	5.717606	-0.024880	2.676381
125.837259	2334.204698	5.722611	-0.024931	2.680620
126.186642	2342.235648	5.727616	-0.025001	2.684874
126.254386	2350.294577	5.732621	-0.025019	2.689118
126.464194	2358.378888	5.737626	-0.025064	2.693377
126.644512	2366.411754	5.742630	-0.025103	2.697601
126.712479	2374.448158	5.747635	-0.025121	2.701813
127.344564	2382.461692	5.752640	-0.025244	2.706042
127.503967	2390.523248	5.757645	-0.025279	2.710259
127.692495	2398.613163	5.762650	-0.025319	2.714487
127.754083	2406.660714	5.767654	-0.025336	2.718678
128.021609	2414.661879	5.772659	-0.025391	2.722851
128.490336	2422.700912	5.777664	-0.025484	2.727050
128.681212	2430.752469	5.782669	-0.025525	2.731231
128.913114	2438.804362	5.787674	-0.025573	2.735409
129.284363	2446.830407	5.792678	-0.025648	2.739576
129.612876	2454.854553	5.797683	-0.025714	2.743732
129.999188	2462.910944	5.802688	-0.025791	2.747903
130.286101	2471.005507	5.807693	-0.025850	2.752080
130.623811	2479.096820	5.812698	-0.025919	2.756253
130.777882	2487.117298	5.817702	-0.025953	2.760372
131.191621	2495.080909	5.822707	-0.026035	2.764471
131.421549	2503.150281	5.827712	-0.026083	2.768607
131.542368	2511.221343	5.832717	-0.026111	2.772731
131.839797	2519.260569	5.837722	-0.026172	2.776843
131.925247	2527.320623	5.842726	-0.026193	2.780948
131.947214	2535.344655	5.847731	-0.026202	2.785024
132.306169	2543.402931	5.852736	-0.026275	2.789131
132.644668	2551.425686	5.857741	-0.026343	2.793213
132.802339	2559.473277	5.862746	-0.026378	2.797291
133.042497	2567.505226	5.867750	-0.026428	2.801360
133.245261	2575.524802	5.872755	-0.026471	2.805414
133.430242	2583.599112	5.877760	-0.026511	2.809490
133.529266	2591.669657	5.882765	-0.026534	2.813552
134.074681	2599.677031	5.887770	-0.026641	2.817602
134.343284	2607.733573	5.892774	-0.026697	2.821656
134.492979	2615.750537	5.897779	-0.026730	2.825677
134.916479	2623.795876	5.902784	-0.026814	2.829721
135.211574	2631.873244	5.907789	-0.026874	2.833769
135.426003	2639.909446	5.912794	-0.026920	2.837786
135.543172	2647.949376	5.917798	-0.026947	2.841793
135.641296	2655.966422	5.922803	-0.026970	2.845783
135.991596	2664.019740	5.927808	-0.027041	2.849798
136.022261	2672.088596	5.932813	-0.027052	2.853798
136.495559	2680.098011	5.937818	-0.027145	2.857788
136.543424	2688.147843	5.942822	-0.027160	2.861768
136.547250	2696.182844	5.947827	-0.027166	2.865733
136.977517	2704.207105	5.952832	-0.027251	2.869711
137.267169	2712.245168	5.957837	-0.027310	2.873682
137.505347	2720.296459	5.962842	-0.027360	2.877651
137.842767	2728.335825	5.967846	-0.027428	2.881615
137.880599	2736.363106	5.972851	-0.027441	2.885550
138.226062	2744.406084	5.977856	-0.027510	2.889505
138.490101	2752.460371	5.982861	-0.027565	2.893455
138.660872	2760.537440	5.987866	-0.027602	2.897406
138.864280	2768.571377	5.992870	-0.027645	2.901332
138.968689	2776.577825	5.997875	-0.027670	2.905235
139.295101	2784.637464	6.002880	-0.027736	2.909169
139.707975	2792.732149	6.007885	-0.027818	2.913120
139.818995	2800.799689	6.012890	-0.027844	2.917036
140.115232	2808.786174	6.017894	-0.027905	2.920918
140.218648	2816.769670	6.022899	-0.027929	2.924783
140.634849	2824.796891	6.027904	-0.028012	2.928680
140.648463	2832.849814	6.032909	-0.028020	2.932563
140.867824	2840.910476	6.037914	-0.028066	2.936455
141.220707	2848.918059	6.042918	-0.028137	2.940324
141.439059	2856.923014	6.047923	-0.028183	2.944180
141.789598	2864.952925	6.052928	-0.028254	2.948049
141.938123	2873.016082	6.057933	-0.028287	2.951918
142.212949	2881.109581	6.062938	-0.028344	2.955803
142.124098	2889.129469	6.067942	-0.028332	2.959630
142.536840	2897.112283	6.072947	-0.028415	2.963459
142.883702	2905.167147	6.077952	-0.028484	2.967315
142.902074	2913.241627	6.082957	-0.028493	2.971157
143.106932	2921.284273	6.087962	-0.028537	2.974990
143.598428	2929.285069	6.092966	-0.028634	2.978812
143.668357	2937.326189	6.097971	-0.028652	2.982626
144.345154	2945.330891	6.102976	-0.028783	2.986450
144.634301	2953.359633	6.107981	-0.028842	2.990260
145.122144	2961.427336	6.112986	-0.028939	2.994093
145.169895	2969.480000	6.117990	-0.028953	2.997893
145.315461	2977.498086	6.122995	-0.028985	3.001676
145.672888	2985.524624	6.128000	-0.029057	3.005469
145.990357	2993.545751	6.133005	-0.029122	3.009252
146.263151	3001.605810	6.138010	-0.029178	3.013047
146.639357	3009.656671	6.143014	-0.029253	3.016838
146.509113	3017.695428	6.148019	-0.029234	3.020593
146.727750	3025.727069	6.153024	-0.029280	3.024358
147.081527	3033.741364	6.158029	-0.029352	3.028116
147.254373	3041.809429	6.163034	-0.029389	3.031886
147.303020	3049.875710	6.168038	-0.029403	3.035644
147.574707	3057.851645	6.173043	-0.029459	3.039367
147.943759	3065.873165	6.178048	-0.029533	3.043110
148.001996	3073.920030	6.183053	-0.029550	3.046846
148.234785	3081.972972	6.188058	-0.029598	3.050588
148.761966	3090.002938	6.193062	-0.029702	3.054330
148.841603	3098.039653	6.198067	-0.029722	3.058048
149.147645	3106.073141	6.203072	-0.029784	3.061771
149.082907	3114.105046	6.208077	-0.029778	3.065471
149.596462	3122.124887	6.213082	-0.029879	3.069188
149.675501	3130.261494	6.218086	-0.029899	3.072934
149.883684	3138.289539	6.223091	-0.029943	3.076632
150.123967	3146.278480	6.228096	-0.029993	3.080309
150.232650	3154.295204	6.233101	-0.030018	3.083988
150.504844	3162.317310	6.238106	-0.030074	3.087672
150.802052	3170.359602	6.243110	-0.030135	3.091363
150.810270	3178.378526	6.248115	-0.030142	3.095025
150.887017	3186.458972	6.253120	-0.030162	3.098714
151.209053	3194.458644	6.258125	-0.030227	3.102373
151.501879	3202.469485	6.263130	-0.030287	3.106031
151.599587	3210.519055	6.268134	-0.030310	3.109694
151.797714	3218.568842	6.273139	-0.030352	3.113357
152.163462	3226.606014	6.278144	-0.030426	3.117018
152.352705	3234.615184	6.283149	-0.030466	3.120653
152.674816	3242.604733	6.288154	-0.030532	3.124282
153.076598	3250.649784	6.293158	-0.030612	3.127934
153.130472	3258.689675	6.298163	-0.030627	3.131565
153.525655	3266.760026	6.303168	-0.030706	3.135220
153.793125	3274.784573	6.308173	-0.030761	3.138845
154.025146	3282.787287	6.313178	-0.030810	3.142454
154.300429	3290.840289	6.318182	-0.030867	3.146083
154.435647	3298.839153	6.323187	-0.030897	3.149678
154.716462	3306.943152	6.328192	-0.030955	3.153322
154.953754	3314.970888	6.333197	-0.031004	3.156926
154.938893	3322.989127	6.338202	-0.031007	3.160510
155.159196	3330.997842	6.343206	-0.031053	3.164096
155.328034	3339.006039	6.348211	-0.031090	3.167676
155.701723	3347.064578	6.353216	-0.031165	3.171283
155.899170	3355.087723	6.358221	-0.031207	3.174862
156.123564	3363.113921	6.363226	-0.031254	3.178440
156.121282	3371.198494	6.368230	-0.031259	3.182030
156.215159	3379.175235	6.373235	-0.031282	3.185572
156.417396	3387.240783	6.378240	-0.031325	3.189154
156.574675	3395.302861	6.383245	-0.031359	3.192729
156.852339	3403.326550	6.388250	-0.031416	3.196288
157.124366	3411.336518	6.393254	-0.031472	3.199836
157.322245	3419.322190	6.398259	-0.031515	3.203367
157.468664	3427.376950	6.403264	-0.031547	3.206922
157.335164	3435.440215	6.408269	-0.031528	3.210465
157.749689	3443.445005	6.413274	-0.031610	3.214002
158.040204	3451.483301	6.418278	-0.031670	3.217543
158.104720	3459.525484	6.423283	-0.031687	3.221074
158.446947	3467.504871	6.428288	-0.031756	3.224584
158.609309	3475.570618	6.433293	-0.031792	3.228121
158.621327	3483.652902	6.438298	-0.031799	3.231655
158.727379	3491.728850	6.443302	-0.031824	3.235187
158.874914	3499.689531	6.448307	-0.031857	3.238665
159.130651	3507.709025	6.453312	-0.031910	3.242170
159.377432	3515.686492	6.458317	-0.031961	3.245653
159.605388	3523.716777	6.463322	-0.032009	3.249154
160.051769	3531.781734	6.468326	-0.032098	3.252675
160.113741	3539.835581	6.473331	-0.032114	3.256172
160.425423	3547.803132	6.478336	-0.032178	3.259638
160.866336	3555.813659	6.483341	-0.032265	3.263123
160.840220	3563.881439	6.488346	-0.032266	3.266612
160.858310	3571.942959	6.493350	-0.032274	3.270095
161.151726	3579.975730	6.498355	-0.032334	3.273573
161.218317	3588.031272	6.503360	-0.032352	3.277049
161.292658	3596.024345	6.508365	-0.032371	3.280494
161.471212	3604.025880	6.513370	-0.032410	3.283943
161.853477	3612.059697	6.518374	-0.032486	3.287410
162.148445	3620.102045	6.523379	-0.032547	3.290874
162.414129	3628.157834	6.528384	-0.032601	3.294339
162.494402	3636.173963	6.533389	-0.032622	3.297776
162.590455	3644.187600	6.538394	-0.032645	3.301209
162.918958	3652.203499	6.543398	-0.032711	3.304648
163.042053	3660.238162	6.548403	-0.032740	3.308084
163.450268	3668.290322	6.553408	-0.032821	3.311534
163.535577	3676.353329	6.558413	-0.032842	3.314974
163.744338	3684.355134	6.563418	-0.032886	3.318388
164.193402	3692.371985	6.568422	-0.032975	3.321814
164.044293	3700.366204	6.573427	-0.032953	3.325204
164.228155	3708.415800	6.578432	-0.032993	3.328627
164.626105	3716.414479	6.583437	-0.033072	3.332033
164.571645	3724.492842	6.588442	-0.033067	3.335452
164.890691	3732.512164	6.593446	-0.033132	3.338857
165.023414	3740.516891	6.598451	-0.033162	3.342245
165.229688	3748.540435	6.603456	-0.033206	3.345640
165.205823	3756.593674	6.608461	-0.033207	3.349036
165.360180	3764.644851	6.613466	-0.033241	3.352434
165.850672	3772.678226	6.618470	-0.033337	3.355833
165.790313	3780.656754	6.623475	-0.033331	3.359186
166.108094	3788.689552	6.628480	-0.033396	3.362572
166.223871	3796.715176	6.633485	-0.033423	3.365944
166.395935	3804.722487	6.638490	-0.033460	3.369307
166.475172	3812.821141	6.643494	-0.033480	3.372701
166.622763	3820.859463	6.648499	-0.033513	3.376070
166.954606	3828.826711	6.653504	-0.033580	3.379411
166.988224	3836.890131	6.658509	-0.033592	3.382780
167.262481	3844.891833	6.663514	-0.033648	3.386127
167.560583	3852.940805	6.668518	-0.033709	3.389491
167.572520	3861.019765	6.673523	-0.033717	3.392855
167.810268	3869.074269	6.678528	-0.033766	3.396213
168.247579	3877.013382	6.683533	-0.033853	3.399527
168.578777	3885.015232	6.688538	-0.033920	3.402860
168.699940	3893.055415	6.693542	-0.033948	3.406198
168.748722	3901.045481	6.698547	-0.033962	3.409509
169.113610	3909.107672	6.703552	-0.034036	3.412858
169.155865	3917.154822	6.708557	-0.034049	3.416186
169.274619	3925.153612	6.713562	-0.034076	3.419494
169.610969	3933.199045	6.718566	-0.034144	3.422825
169.938668	3941.182724	6.723571	-0.034210	3.426128
170.032862	3949.233624	6.728576	-0.034233	3.429446
170.111310	3957.276960	6.733581	-0.034253	3.432758
170.293108	3965.321189	6.738586	-0.034293	3.436071
170.676685	3973.294458	6.743590	-0.034369	3.439357
170.696277	3981.327203	6.748595	-0.034378	3.442653
171.156421	3989.367002	6.753600	-0.034469	3.445964
171.303058	3997.389762	6.758605	-0.034502	3.449253
171.261328	4005.442328	6.763610	-0.034499	3.452546
171.610696	4013.500133	6.768614	-0.034570	3.455850
171.702851	4021.504611	6.773619	-0.034592	3.459121
171.758946	4029.527261	6.778624	-0.034608	3.462395
171.950973	4037.534412	6.783629	-0.034649	3.465664
172.190192	4045.569243	6.788634	-0.034699	3.468943
172.345148	4053.647678	6.793638	-0.034733	3.472233
172.311057	4061.677361	6.798643	-0.034732	3.475495
172.656579	4069.658379	6.803648	-0.034802	3.478746
172.818513	4077.689247	6.808653	-0.034837	3.482008
172.808734	4085.678036	6.813658	-0.034841	3.485245
173.078392	4093.717120	6.818662	-0.034896	3.488507
173.206199	4101.734043	6.823667	-0.034926	3.491754
173.403703	4109.770826	6.828672	-0.034968	3.495007
173.466789	4117.790856	6.833677	-0.034985	3.498246
173.850120	4125.785706	6.838682	-0.035061	3.501483
174.078110	4133.828870	6.843686	-0.035109	3.504731
174.175160	4141.849391	6.848691	-0.035133	3.507962
174.476852	4149.905833	6.853696	-0.035194	3.511212
174.492799	4157.946797	6.858701	-0.035202	3.514443
174.683403	4165.963866	6.863706	-0.035243	3.517667
175.052921	4173.979354	6.868710	-0.035317	3.520893
175.163045	4181.966062	6.873715	-0.035343	3.524096
175.400097	4190.028447	6.878720	-0.035393	3.527331
175.512721	4198.053139	6.883725	-0.035419	3.530544
175.672402	4206.069126	6.888730	-0.035454	3.533752
175.894674	4214.121386	6.893734	-0.035501	3.536973
175.945981	4222.127428	6.898739	-0.035516	3.540168
176.094121	4230.154610	6.903744	-0.035549	3.543371
176.234260	4238.181101	6.908749	-0.035580	3.546571
176.192005	4246.237987	6.913754	-0.035578	3.549774
176.546477	4254.360550	6.918758	-0.035649	3.553013
176.737120	4262.373877	6.923763	-0.035690	3.556200
177.037608	4270.309953	6.928768	-0.035751	3.559357
177.103755	4278.320225	6.933773	-0.035769	3.562534
177.287928	4286.321866	6.938778	-0.035808	3.565707
177.452091	4294.359834	6.943782	-0.035844	3.568892
177.762579	4302.357961	6.948787	-0.035907	3.572062
177.984127	4310.414943	6.953792	-0.035954	3.575251
178.126121	4318.401919	6.958797	-0.035986	3.578406
178.036301	4326.466795	6.963802	-0.035974	3.581583
178.374150	4334.443466	6.968806	-0.036042	3.584734
178.559834	4342.481213	6.973811	-0.036082	3.587902
178.772370	4350.512297	6.978816	-0.036127	3.591066
178.979409	4358.549373	6.983821	-0.036171	3.594229
179.303467	4366.543828	6.988826	-0.036237	3.597375
179.442404	4374.565886	6.993830	-0.036268	3.600525
179.669505	4382.563218	6.998835	-0.036316	3.603664
179.743193	4390.645607	7.003840	-0.036335	3.606830
180.023837	4398.603809	7.008845	-0.036392	3.609950
180.117027	4406.675855	7.013850	-0.036415	3.613107
180.272656	4414.760192	7.018854	-0.036449	3.616267
180.354745	4422.732751	7.023859	-0.036470	3.619379
180.621300	4430.730491	7.028864	-0.036525	3.622503
180.636739	4438.763313	7.033869	-0.036533	3.625632
180.913923	4446.800826	7.038874	-0.036590	3.628766
181.124784	4454.879781	7.043878	-0.036635	3.631912
181.247286	4462.889155	7.048883	-0.036663	3.635026
181.545835	4470.885194	7.053888	-0.036724	3.638137
181.813225	4478.925015	7.058893	-0.036779	3.641261
181.905969	4486.896032	7.063898	-0.036801	3.644351
182.061963	4494.962316	7.068902	-0.036836	3.647477
182.373364	4502.939317	7.073907	-0.036899	3.650570
182.721000	4511.001590	7.078912	-0.036969	3.653694
182.770798	4519.053221	7.083917	-0.036984	3.656804
183.039369	4527.036117	7.088922	-0.037039	3.659890
183.351693	4535.078833	7.093926	-0.037103	3.662998
183.274446	4543.114320	7.098931	-0.037094	3.666090
183.146238	4551.155130	7.103936	-0.037075	3.669180
183.527250	4559.172483	7.108941	-0.037151	3.672272
183.628365	4567.184639	7.113946	-0.037175	3.675351
183.784551	4575.214534	7.118950	-0.037210	3.678437
184.134601	4583.193522	7.123955	-0.037280	3.681505
184.363197	4591.160498	7.128960	-0.037328	3.684563
184.660429	4599.218592	7.133965	-0.037389	3.687655
184.849046	4607.260551	7.138970	-0.037429	3.690736
185.118768	4615.341573	7.143974	-0.037485	3.693831
185.316957	4623.336037	7.148979	-0.037527	3.696888
185.592074	4631.331357	7.153984	-0.037584	3.699945
185.719949	4639.351228	7.158989	-0.037613	3.703005
185.946511	4647.375472	7.163994	-0.037660	3.706067
186.176671	4655.416075	7.168998	-0.037709	3.709132
186.209510	4663.485245	7.174003	-0.037720	3.712201
186.657678	4671.540894	7.179008	-0.037809	3.715273
186.818388	4679.510006	7.184013	-0.037844	3.718302
186.912690	4687.507246	7.189018	-0.037867	3.721337
187.158536	4695.497253	7.194022	-0.037918	3.724371
187.250026	4703.516104	7.199027	-0.037940	3.727410
187.309327	4711.558451	7.204032	-0.037957	3.730454
187.774291	4719.602353	7.209037	-0.038049	3.733506
187.862862	4727.616464	7.214042	-0.038071	3.736536
187.768381	4735.654444	7.219046	-0.038058	3.739567
188.007150	4743.645692	7.224051	-0.038108	3.742586
188.284597	4751.667610	7.229056	-0.038165	3.745616
188.300736	4759.687566	7.234061	-0.038173	3.748635
188.497720	4767.749249	7.239066	-0.038215	3.751673
188.746458	4775.807704	7.244070	-0.038267	3.754708
188.880784	4783.788394	7.249075	-0.038297	3.757708
189.124013	4791.803774	7.254080	-0.038348	3.760722
189.335415	4799.791836	7.259085	-0.038393	3.763722
189.477665	4807.836452	7.264090	-0.038425	3.766740
189.413569	4815.898512	7.269094	-0.038418	3.769756
189.365215	4823.920132	7.274099	-0.038414	3.772756
189.699047	4831.951686	7.279104	-0.038482	3.775766
189.959052	4839.930709	7.284109	-0.038535	3.778752
190.055474	4847.958659	7.289114	-0.038559	3.781750
190.491644	4855.950849	7.294118	-0.038645	3.784740
190.581313	4864.018078	7.299123	-0.038667	3.787747
190.673003	4872.039632	7.304128	-0.038690	3.790736
191.032062	4880.097841	7.309133	-0.038762	3.793741
191.279992	4888.113735	7.314138	-0.038813	3.796726
191.343112	4896.101560	7.319142	-0.038831	3.799694
191.247835	4904.112566	7.324147	-0.038818	3.802665
191.591533	4912.102355	7.329152	-0.038887	3.805635
191.900052	4920.116617	7.334157	-0.038950	3.808612
192.026117	4928.152143	7.339162	-0.038979	3.811589
192.508407	4936.185983	7.344166	-0.039074	3.814572
192.624281	4944.210369	7.349171	-0.039101	3.817541
192.989522	4952.208910	7.354176	-0.039174	3.820503
193.028940	4960.228334	7.359181	-0.039187	3.823463
193.342928	4968.259432	7.364186	-0.039251	3.826432
193.329025	4976.296148	7.369190	-0.039254	3.829393
193.555290	4984.330501	7.374195	-0.039301	3.832356
193.722772	4992.332919	7.379200	-0.039338	3.835304
193.842365	5000.342581	7.384205	-0.039365	3.838251
193.899394	5008.330528	7.389210	-0.039381	3.841187
194.217604	5016.394184	7.394214	-0.039446	3.844153
194.397173	5024.386822	7.399219	-0.039484	3.847088
194.341102	5032.438841	7.404224	-0.039479	3.850038
194.505856	5040.487306	7.409229	-0.039515	3.852989
194.794463	5048.490781	7.414234	-0.039574	3.855924
194.956589	5056.522839	7.419238	-0.039610	3.858864
194.947590	5064.543158	7.424243	-0.039614	3.861795
195.215423	5072.553547	7.429248	-0.039669	3.864725
195.452745	5080.613753	7.434253	-0.039718	3.867670
195.365501	5088.597631	7.439258	-0.039707	3.870579
195.627520	5096.869497	7.444262	-0.039762	3.873597
195.808010	5104.827135	7.449267	-0.039801	3.876497
196.061409	5112.713903	7.454272	-0.039853	3.879371
196.113721	5120.728271	7.459277	-0.039868	3.882284
196.390249	5128.721231	7.464282	-0.039925	3.885192
196.617925	5136.756470	7.469286	-0.039973	3.888113
196.666411	5144.782383	7.474291	-0.039987	3.891024
196.990940	5152.833364	7.479296	-0.040053	3.893948
196.974213	5160.849852	7.484301	-0.040055	3.896850
197.092132	5168.765119	7.489306	-0.040082	3.899716
197.258757	5176.836626	7.494310	-0.040119	3.902637
197.545681	5184.845750	7.499315	-0.040177	3.905536
197.773613	5192.864015	7.504320	-0.040225	3.908435
198.039975	5200.879424	7.509325	-0.040280	3.911331
198.186532	5208.939991	7.514330	-0.040313	3.914239
198.225372	5216.963588	7.519334	-0.040325	3.917130
198.370988	5224.892228	7.524339	-0.040358	3.919986
198.814641	5232.958307	7.529344	-0.040446	3.922895
199.113356	5241.000553	7.534349	-0.040507	3.925791
199.034998	5249.005298	7.539354	-0.040497	3.928664
199.325892	5257.047778	7.544358	-0.040557	3.931555
199.510351	5265.035450	7.549363	-0.040596	3.934423
199.608337	5273.091751	7.554368	-0.040620	3.937311
199.678020	5281.079539	7.559373	-0.040638	3.940173
199.758742	5289.079605	7.564378	-0.040659	3.943036
199.855049	5297.114461	7.569382	-0.040682	3.945911
199.949856	5305.124702	7.574387	-0.040705	3.948774
200.173187	5313.147635	7.579392	-0.040752	3.951642
200.408795	5321.210919	7.584397	-0.040801	3.954523
200.445926	5329.195211	7.589402	-0.040813	3.957370
200.504684	5337.198258	7.594406	-0.040830	3.960222
200.870888	5345.183521	7.599411	-0.040903	3.963071
200.951187	5353.244601	7.604416	-0.040923	3.965940
200.908834	5361.277005	7.609421	-0.040921	3.968794
201.219798	5369.270229	7.614426	-0.040984	3.971639
201.571953	5377.314004	7.619430	-0.041055	3.974500
201.588034	5385.350539	7.624435	-0.041063	3.977350
201.629533	5393.325570	7.629440	-0.041076	3.980178
201.834244	5401.387718	7.634445	-0.041120	3.983036
202.048457	5409.366184	7.639450	-0.041165	3.985864
202.174874	5417.432198	7.644454	-0.041194	3.988718
202.348864	5425.457667	7.649459	-0.041232	3.991558
202.508578	5433.475439	7.654464	-0.041267	3.994392
202.740857	5441.520434	7.659469	-0.041315	3.997235
202.781884	5449.499401	7.664474	-0.041328	4.000049
202.956405	5457.553274	7.669478	-0.041366	4.002890
202.870825	5465.555546	7.674483	-0.041355	4.005707
203.141945	5473.558886	7.679488	-0.041411	4.008528
203.400038	5481.597877	7.684493	-0.041465	4.011359
203.489732	5489.643076	7.689498	-0.041487	4.014187
203.703823	5497.660003	7.694502	-0.041532	4.017006
203.764112	5505.633397	7.699507	-0.041548	4.019805
203.977008	5513.700060	7.704512	-0.041593	4.022636
204.217764	5521.707111	7.709517	-0.041643	4.025446
204.260488	5529.702654	7.714522	-0.041657	4.028246
204.592903	5537.775972	7.719526	-0.041724	4.031077
204.672449	5545.887498	7.724531	-0.041744	4.033914
204.962543	5553.870571	7.729536	-0.041804	4.036708
205.320288	5561.783953	7.734541	-0.041875	4.039477
205.630683	5569.808766	7.739546	-0.041939	4.042281
205.718203	5577.816526	7.744550	-0.041960	4.045075
205.842817	5585.821124	7.749555	-0.041989	4.047866
206.094283	5593.844796	7.754560	-0.042041	4.050664
206.165659	5601.910403	7.759565	-0.042059	4.053471
206.566486	5609.891542	7.764570	-0.042139	4.056252
206.928583	5617.905109	7.769574	-0.042212	4.059042
206.847838	5625.937267	7.774579	-0.042202	4.061830
206.995621	5633.901609	7.779584	-0.042235	4.064596
207.187970	5641.970489	7.784589	-0.042276	4.067397
207.084860	5649.984967	7.789594	-0.042263	4.070172
207.207723	5658.063350	7.794598	-0.042291	4.072972
207.541106	5666.062135	7.799603	-0.042358	4.075744
207.878298	5674.058232	7.804608	-0.042426	4.078514
207.766158	5682.077885	7.809613	-0.042411	4.081284
207.762786	5690.039835	7.814618	-0.042415	4.084033
208.300443	5698.126901	7.819622	-0.042521	4.086832
208.293052	5706.061918	7.824627	-0.042525	4.089568
208.351994	5714.161861	7.829632	-0.042541	4.092360
208.660006	5722.171502	7.834637	-0.042604	4.095123
208.883755	5730.183606	7.839642	-0.042651	4.097884
208.925281	5738.221874	7.844646	-0.042664	4.100649
209.027597	5746.197833	7.849651	-0.042688	4.103391
209.241194	5754.198562	7.854656	-0.042733	4.106142
209.269860	5762.273662	7.859661	-0.042744	4.108914
209.207327	5770.319447	7.864666	-0.042738	4.111673
209.422402	5778.392050	7.869670	-0.042783	4.114443
209.492725	5786.391735	7.874675	-0.042802	4.117184
209.602782	5794.341478	7.879680	-0.042827	4.119907
209.841660	5802.357488	7.884685	-0.042877	4.122652
210.056873	5810.315871	7.889690	-0.042923	4.125375
210.140757	5818.400527	7.894694	-0.042943	4.128138
210.247324	5826.389188	7.899699	-0.042969	4.130867
210.414710	5834.464276	7.904704	-0.043005	4.133624
210.816701	5842.524453	7.909709	-0.043085	4.136377
210.526629	5850.474784	7.914714	-0.043037	4.139082
210.835586	5858.536302	7.919718	-0.043100	4.141831
211.110620	5866.484278	7.924723	-0.043156	4.144539
211.149729	5874.539589	7.929728	-0.043169	4.147278
211.263849	5882.563610	7.934733	-0.043195	4.150006
211.429248	5890.577378	7.939738	-0.043231	4.152729
211.630992	5898.633872	7.944742	-0.043274	4.155466
211.790612	5906.644732	7.949747	-0.043309	4.158184
212.040924	5914.612639	7.954752	-0.043361	4.160888
212.277001	5922.620442	7.959757	-0.043411	4.163603
212.184267	5930.694571	7.964762	-0.043399	4.166334
212.439416	5938.680045	7.969766	-0.043451	4.169038
212.575734	5946.686817	7.974771	-0.043482	4.171746
212.799020	5954.726461	7.979776	-0.043529	4.174465
212.833948	5962.771220	7.984781	-0.043541	4.177181
212.881320	5970.726403	7.989786	-0.043555	4.179865
213.136631	5978.792918	7.994790	-0.043608	4.182588
213.224391	5986.758105	7.999795	-0.043630	4.185272
213.279214	5994.792589	8.004800	-0.043645	4.187978
213.526107	6002.853956	8.009805	-0.043696	4.190693
213.576691	6010.931590	8.014810	-0.043711	4.193410
213.853112	6018.985000	8.019814	-0.043768	4.196119
213.956739	6026.878091	8.024819	-0.043793	4.198771
214.144483	6034.907574	8.029824	-0.043833	4.201468
214.241083	6042.877175	8.034829	-0.043856	4.204142
214.441393	6050.901785	8.039834	-0.043899	4.206834
214.568302	6058.924566	8.044838	-0.043928	4.209522
214.726467	6066.961840	8.049843	-0.043963	4.212214
214.962713	6074.996349	8.054848	-0.044012	4.214905
215.195911	6082.996019	8.059853	-0.044061	4.217582
215.301088	6090.962661	8.064858	-0.044085	4.220244
215.529760	6099.027970	8.069862	-0.044133	4.222940
215.518575	6107.006443	8.074867	-0.044137	4.225602
215.632502	6115.033087	8.079872	-0.044163	4.228279
215.706255	6123.093228	8.084877	-0.044182	4.230966
215.894822	6131.112053	8.089882	-0.044223	4.233639
216.134663	6139.182402	8.094886	-0.044273	4.236327
216.015854	6147.131199	8.099891	-0.044256	4.238970
216.350838	6155.136799	8.104896	-0.044324	4.241634
216.515921	6163.098804	8.109901	-0.044360	4.244281
216.631779	6171.172594	8.114906	-0.044387	4.246962
216.872946	6179.178387	8.119910	-0.044437	4.249620
217.102307	6187.233895	8.124915	-0.044485	4.252294
217.169219	6195.242498	8.129920	-0.044503	4.254948
217.492368	6203.320803	8.134925	-0.044568	4.257626
217.673896	6211.240205	8.139930	-0.044607	4.260248
217.875071	6219.332117	8.144934	-0.044650	4.262926
217.837189	6227.303325	8.149939	-0.044648	4.265561
217.940660	6235.375914	8.154944	-0.044673	4.268228
218.140620	6243.358346	8.159949	-0.044715	4.270865
218.200163	6251.413846	8.164954	-0.044732	4.273523
218.350172	6259.483410	8.169958	-0.044765	4.276185
218.503385	6267.430982	8.174963	-0.044799	4.278805
218.744786	6275.444779	8.179968	-0.044849	4.281446
218.796691	6283.444718	8.184973	-0.044864	4.284079
218.970340	6291.481673	8.189978	-0.044902	4.286724
219.263070	6299.456079	8.194982	-0.044962	4.289347
219.147968	6307.551149	8.199987	-0.044946	4.292005
219.383828	6315.523638	8.204992	-0.044995	4.294624
219.403772	6323.620603	8.209997	-0.045004	4.297281
219.651202	6331.536103	8.215002	-0.045055	4.299878
219.603238	6339.580828	8.220006	-0.045052	4.302513
219.920253	6347.593161	8.225011	-0.045116	4.305140
220.052941	6355.581481	8.230016	-0.045146	4.307755
220.363316	6363.634525	8.235021	-0.045209	4.310391
220.398504	6371.679924	8.240026	-0.045221	4.313021
220.582520	6379.711527	8.245030	-0.045261	4.315646
220.589110	6387.709112	8.250035	-0.045267	4.318257
220.727221	6395.675063	8.255040	-0.045298	4.320857
220.989909	6403.699583	8.260045	-0.045353	4.323475
220.886515	6411.705616	8.265050	-0.045339	4.326084
221.265784	6419.738385	8.270054	-0.045415	4.328702
221.364755	6427.793832	8.275059	-0.045438	4.331325
221.501601	6435.799620	8.280064	-0.045469	4.333930
221.711230	6443.833701	8.285069	-0.045514	4.336543
221.475750	6451.800500	8.290074	-0.045475	4.339130
221.913188	6459.830851	8.295078	-0.045562	4.341740
221.933797	6467.812384	8.300083	-0.045571	4.344330
222.057584	6475.851449	8.305088	-0.045599	4.346938
222.327222	6483.866386	8.310093	-0.045655	4.349537
222.308938	6491.904626	8.315098	-0.045657	4.352140
222.574010	6500.026869	8.320102	-0.045712	4.354771
222.670501	6508.012701	8.325107	-0.045735	4.357355
223.092954	6515.930230	8.330112	-0.045819	4.359918
223.009273	6523.955279	8.335117	-0.045808	4.362511
222.972176	6531.919380	8.340122	-0.045807	4.365082
223.199939	6539.967276	8.345126	-0.045855	4.367681
223.380173	6547.979333	8.350131	-0.045893	4.370266
223.581449	6556.042322	8.355136	-0.045936	4.372867
223.738662	6564.089691	8.360141	-0.045971	4.375460
223.773739	6572.047157	8.365146	-0.045983	4.378022
223.833270	6580.061269	8.370150	-0.045999	4.380601
224.109957	6588.068456	8.375155	-0.046056	4.383178
224.338504	6596.057038	8.380160	-0.046104	4.385747
224.371754	6604.147182	8.385165	-0.046115	4.388345
224.593835	6612.119192	8.390170	-0.046162	4.390906
224.697650	6620.198251	8.395174	-0.046187	4.393498
224.716347	6628.231960	8.400179	-0.046196	4.396074
224.926803	6636.187253	8.405184	-0.046240	4.398625
225.026046	6644.270022	8.410189	-0.046264	4.401214
225.389200	6652.191289	8.415194	-0.046337	4.403751
225.206750	6660.254039	8.420198	-0.046308	4.406329
225.230625	6668.245844	8.425203	-0.046318	4.408884
225.607966	6676.267971	8.430208	-0.046394	4.411449
225.753058	6684.342576	8.435213	-0.046426	4.414028
225.773176	6692.329960	8.440218	-0.046435	4.416577
226.054643	6700.356167	8.445222	-0.046493	4.419139
226.149400	6708.373312	8.450227	-0.046516	4.421695
226.316258	6716.314665	8.455232	-0.046552	4.424225
226.662279	6724.400228	8.460237	-0.046622	4.426801
226.878942	6732.415972	8.465242	-0.046668	4.429353
227.164944	6740.463918	8.470246	-0.046726	4.431914
227.136410	6748.496515	8.475251	-0.046726	4.434466
227.198532	6756.503965	8.480256	-0.046743	4.437010
227.640800	6764.508858	8.485261	-0.046831	4.439553
227.580723	6772.511540	8.490266	-0.046825	4.442092
227.858467	6780.456174	8.495270	-0.046882	4.444613
227.868124	6788.542974	8.500275	-0.046889	4.447175
227.930847	6796.550941	8.505280	-0.046906	4.449712
228.037277	6804.631025	8.510285	-0.046931	4.452270
228.415215	6812.594930	8.515290	-0.047007	4.454791
228.544994	6820.658426	8.520294	-0.047036	4.457341
228.576548	6828.626993	8.525299	-0.047048	4.459860
228.787697	6836.586067	8.530304	-0.047092	4.462374
228.814372	6844.631044	8.535309	-0.047102	4.464913
228.940783	6852.609179	8.540314	-0.047131	4.467431
229.066400	6860.731542	8.545318	-0.047160	4.469992
229.346074	6868.716164	8.550323	-0.047217	4.472509
229.360905	6876.709307	8.555328	-0.047226	4.475026
229.587633	6884.776113	8.560333	-0.047273	4.477566
229.886814	6892.703869	8.565338	-0.047334	4.480061
230.150416	6900.766667	8.570343	-0.047389	4.482596
230.211335	6908.773598	8.575347	-0.047405	4.485113
230.280410	6916.792931	8.580352	-0.047423	4.487631
230.451188	6924.796899	8.585357	-0.047460	4.490144
230.583799	6932.814754	8.590362	-0.047491	4.492659
230.827495	6940.868986	8.595367	-0.047541	4.495185
230.876605	6948.873836	8.600371	-0.047556	4.497693
231.023690	6956.843401	8.605376	-0.047588	4.500189
231.167653	6964.896312	8.610381	-0.047621	4.502710
231.339522	6972.865700	8.615386	-0.047658	4.505203
231.706344	6980.928832	8.620391	-0.047732	4.507725
231.694700	6988.933795	8.625395	-0.047735	4.510226
232.045382	6996.975280	8.630400	-0.047805	4.512738
232.355292	7005.078751	8.635405	-0.047868	4.515267
232.408348	7013.041694	8.640410	-0.047884	4.517751
232.508356	7020.995673	8.645415	-0.047907	4.520231
232.777912	7028.996930	8.650419	-0.047963	4.522725
232.649484	7036.969442	8.655424	-0.047944	4.525207
232.678282	7045.036513	8.660429	-0.047955	4.527718
232.846182	7052.979642	8.665434	-0.047992	4.530189
233.125072	7061.076132	8.670439	-0.048049	4.532706
233.162182	7069.081278	8.675443	-0.048061	4.535193
233.544241	7077.102804	8.680448	-0.048138	4.537685
233.612177	7085.095545	8.685453	-0.048156	4.540166
233.643598	7093.117064	8.690458	-0.048167	4.542654
233.824872	7101.108928	8.695463	-0.048206	4.545132
234.061124	7109.186576	8.700467	-0.048255	4.547635
234.250741	7117.129852	8.705472	-0.048296	4.550095
234.433526	7125.228891	8.710477	-0.048335	4.552602
234.605155	7133.229554	8.715482	-0.048372	4.555078
234.776424	7141.310402	8.720487	-0.048410	4.557576
234.634989	7149.219255	8.725491	-0.048389	4.560020
234.621689	7157.263221	8.730496	-0.048392	4.562504
235.054826	7165.242005	8.735501	-0.048477	4.564967
235.155255	7173.262981	8.740506	-0.048501	4.567442
235.261673	7181.294411	8.745511	-0.048527	4.569918
235.432967	7189.375629	8.750515	-0.048564	4.572408
235.524433	7197.344978	8.755520	-0.048586	4.574863
235.662364	7205.399672	8.760525	-0.048617	4.577342
235.708971	7213.341304	8.765530	-0.048631	4.579786
235.995958	7221.489696	8.770535	-0.048690	4.582291
236.021566	7229.412632	8.775539	-0.048700	4.584726
236.081625	7237.455626	8.780544	-0.048717	4.587197
236.209359	7245.467245	8.785549	-0.048746	4.589656
236.258453	7253.469115	8.790554	-0.048760	4.592111
236.411376	7261.559647	8.795559	-0.048794	4.594592
236.733958	7269.560631	8.800563	-0.048859	4.597045
236.785029	7277.476652	8.805568	-0.048874	4.599470
236.981319	7285.572165	8.810573	-0.048916	4.601948
237.142750	7293.477229	8.815578	-0.048951	4.604367
237.364947	7301.550877	8.820583	-0.048998	4.606836
237.483892	7309.558507	8.825587	-0.049026	4.609284
237.572863	7317.597033	8.830592	-0.049048	4.611740
237.875445	7325.623503	8.835597	-0.049109	4.614190
238.063730	7333.648215	8.840602	-0.049150	4.616639
237.840301	7341.652576	8.845607	-0.049113	4.619081
238.173804	7349.669559	8.850611	-0.049181	4.621525
238.107575	7357.603531	8.855616	-0.049174	4.623942
238.170092	7365.692496	8.860621	-0.049191	4.626405
238.192485	7373.658533	8.865626	-0.049200	4.628830
238.822018	7381.731162	8.870631	-0.049323	4.631285
238.959099	7389.781931	8.875635	-0.049354	4.633733
239.110556	7397.819572	8.880640	-0.049387	4.636175
239.328473	7405.776299	8.885645	-0.049433	4.638592
239.292210	7413.771726	8.890650	-0.049432	4.641019
239.543381	7421.770945	8.895655	-0.049484	4.643446
239.704911	7429.834998	8.900659	-0.049519	4.645891
239.735943	7437.810291	8.905664	-0.049530	4.648308
239.906377	7445.837572	8.910669	-0.049567	4.650739
240.003462	7453.878190	8.915674	-0.049591	4.653173
240.305943	7461.888635	8.920679	-0.049652	4.655597
240.106984	7469.915094	8.925683	-0.049621	4.658025
240.183948	7477.858852	8.930688	-0.049640	4.660426
240.469255	7485.948109	8.935693	-0.049699	4.662869
240.650027	7493.911004	8.940698	-0.049738	4.665274
240.691139	7501.940618	8.945703	-0.049751	4.667697
240.866934	7509.940855	8.950707	-0.049789	4.670110
240.925182	7518.029704	8.955712	-0.049805	4.672549
241.280767	7526.144956	8.960717	-0.049877	4.674993
241.264159	7534.063669	8.965722	-0.049879	4.677378
241.469462	7542.023880	8.970727	-0.049922	4.679774
241.714597	7550.078773	8.975731	-0.049973	4.682197
241.523615	7557.951707	8.980736	-0.049943	4.684565
241.707310	7566.097741	8.985741	-0.049983	4.687013
241.700443	7574.032828	8.990746	-0.049987	4.689396
242.002115	7582.131946	8.995751	-0.050048	4.691828
242.338304	7590.107608	9.000755	-0.050116	4.694220
242.311832	7598.142377	9.005760	-0.050116	4.696630
242.203293	7606.121341	9.010765	-0.050101	4.699022
242.395663	7614.124134	9.015770	-0.050143	4.701420
242.779693	7622.188767	9.020775	-0.050219	4.703834
242.785224	7630.181903	9.025779	-0.050226	4.706226
242.895184	7638.196601	9.030784	-0.050252	4.708624
242.991787	7646.240398	9.035789	-0.050275	4.711028
243.401423	7654.264694	9.040794	-0.050357	4.713426
243.569223	7662.266195	9.045799	-0.050393	4.715815
243.549132	7670.274457	9.050803	-0.050395	4.718206
243.552614	7678.231514	9.055808	-0.050401	4.720580
243.869662	7686.316764	9.060813	-0.050465	4.722991
243.920673	7694.302299	9.065818	-0.050480	4.725371
244.228390	7702.328800	9.070823	-0.050542	4.727761
244.450340	7710.360796	9.075827	-0.050589	4.730153
244.396450	7718.384901	9.080832	-0.050584	4.732541
244.585022	7726.432180	9.085837	-0.050625	4.734934
244.569020	7734.424883	9.090842	-0.050627	4.737311
244.718350	7742.426412	9.095847	-0.050660	4.739688
244.710388	7750.427263	9.100851	-0.050664	4.742065
245.026569	7758.393431	9.105856	-0.050728	4.744429
245.208122	7766.500142	9.110861	-0.050768	4.746833
245.090684	7774.454079	9.115866	-0.050751	4.749193
245.351218	7782.540403	9.120871	-0.050805	4.751589
245.652942	7790.579731	9.125875	-0.050866	4.753970
245.608553	7798.546507	9.130880	-0.050863	4.756329
245.678554	7806.540711	9.135885	-0.050882	4.758695
246.031583	7814.517982	9.140890	-0.050953	4.761054
246.226391	7822.542872	9.145895	-0.050994	4.763426
246.254246	7830.534944	9.150899	-0.051005	4.765787
246.258319	7838.600480	9.155904	-0.051011	4.768170
246.689595	7846.617249	9.160909	-0.051097	4.770535
246.512629	7854.639939	9.165914	-0.051069	4.772903
246.694401	7862.646844	9.170919	-0.051108	4.775264
246.768705	7870.661675	9.175923	-0.051127	4.777626
246.857562	7878.598035	9.180928	-0.051149	4.779964
247.097327	7886.682454	9.185933	-0.051199	4.782344
247.248536	7894.648841	9.190938	-0.051233	4.784689
247.552459	7902.733839	9.195943	-0.051295	4.787066
247.701671	7910.716724	9.200947	-0.051328	4.789413
247.585891	7918.735924	9.205952	-0.051311	4.791770
247.716133	7926.809376	9.210957	-0.051341	4.794141
247.721774	7934.830812	9.215962	-0.051347	4.796497
248.033710	7942.767125	9.220967	-0.051411	4.798824
248.401265	7950.793423	9.225971	-0.051485	4.801177
248.423147	7958.792962	9.230976	-0.051494	4.803522
248.514887	7966.811361	9.235981	-0.051516	4.805872
248.642577	7974.805504	9.240986	-0.051545	4.808213
248.729912	7982.907495	9.245991	-0.051567	4.810584
248.856735	7990.295933	9.250995	-0.051596	4.812745
248.887257	7994.741837	9.256000	-0.051604	4.814046

249.062037	7997.238477	9.261005	-0.051639	4.814775
249.093965	7998.438003	9.266010	-0.051645	4.815126
249.048882	7998.930571	9.271015	-0.051637	4.815270
249.161406	7999.955344	9.276019	-0.051659	4.815569
249.466740	7999.934697	9.281024	-0.051716	4.815562
249.751039	7999.958556	9.286029	-0.051769	4.815567
249.526524	7999.934620	9.291034	-0.051727	4.815561
249.680987	7999.957433	9.296039	-0.051756	4.815567
249.744237	7999.955269	9.301043	-0.051768	4.815566
249.595603	7999.958196	9.306048	-0.051741	4.815568
249.861013	7999.974274	9.311053	-0.051790	4.815571
249.916524	7999.952762	9.316058	-0.051801	4.815565
249.808139	7999.968091	9.321063	-0.051781	4.815570
249.973025	7999.954768	9.326067	-0.051811	4.815565
250.006867	7999.978821	9.331072	-0.051818	4.815572
250.087597	7999.982280	9.336077	-0.051833	4.815572
250.106473	7999.948426	9.341082	-0.051836	4.815562
250.363815	7999.956898	9.346087	-0.051884	4.815564
250.302940	7999.976204	9.351091	-0.051873	4.815570
250.198534	7999.970241	9.356096	-0.051854	4.815568
250.539616	7999.983281	9.361101	-0.051918	4.815571
250.425962	7999.969692	9.366106	-0.051896	4.815567
250.377093	7999.987059	9.371111	-0.051888	4.815572
250.334496	7999.963949	9.376115	-0.051880	4.815566
250.475195	7999.959843	9.381120	-0.051906	4.815564
250.542056	7999.996180	9.386125	-0.051919	4.815574
250.418855	7999.970689	9.391130	-0.051896	4.815567
250.700104	8000.005180	9.396135	-0.051948	4.815576
250.641010	7999.994615	9.401139	-0.051937	4.815573
250.510665	7999.981822	9.406144	-0.051913	4.815570
250.643995	7999.972257	9.411149	-0.051938	4.815567
250.432664	7999.946399	9.416154	-0.051899	4.815560
250.458977	7999.981007	9.421159	-0.051904	4.815570
250.454268	7999.986279	9.426163	-0.051903	4.815572
250.488431	7999.970827	9.431168	-0.051909	4.815567
250.539814	7999.983419	9.436173	-0.051919	4.815571
250.444427	7999.967992	9.441178	-0.051901	4.815567
250.467213	7999.969440	9.446183	-0.051906	4.815567
250.568235	7999.961484	9.451187	-0.051925	4.815564
250.521653	7999.984227	9.456192	-0.051916	4.815571
250.696860	7999.993497	9.461197	-0.051949	4.815573
250.649207	7999.962830	9.466202	-0.051940	4.815564
250.873305	7999.970762	9.471207	-0.051982	4.815565
250.712872	7999.969224	9.476211	-0.051952	4.815566
250.806962	7999.980377	9.481216	-0.051970	4.815568
250.807272	7999.996409	9.486221	-0.051970	4.815573
250.875009	7999.969757	9.491226	-0.051983	4.815565
250.973920	7999.995939	9.496231	-0.052001	4.815572
250.960630	7999.997867	9.501235	-0.051999	4.815573
250.686303	7999.968845	9.506240	-0.051948	4.815566
250.926079	7999.996254	9.511245	-0.051993	4.815572
250.971031	7999.982045	9.516250	-0.052001	4.815568
250.974912	8000.010950	9.521255	-0.052002	4.815577
250.899805	8000.002260	9.526259	-0.051988	4.815574
250.879075	7999.996592	9.531264	-0.051984	4.815573
250.811606	8000.043555	9.536269	-0.051972	4.815587
250.637475	7999.995877	9.541274	-0.051939	4.815574
250.773551	7999.994899	9.546279	-0.051965	4.815573
250.903124	7999.988477	9.551283	-0.051989	4.815570
250.744535	7999.976291	9.556288	-0.051960	4.815567
250.880589	7999.989195	9.561293	-0.051985	4.815571
250.929498	7999.997476	9.566298	-0.051994	4.815573
250.778065	8000.014239	9.571303	-0.051966	4.815578
250.841509	7999.993925	9.576307	-0.051978	4.815572
250.921970	7999.992041	9.581312	-0.051993	4.815571
250.900806	7999.990638	9.586317	-0.051989	4.815571
250.741794	7999.972038	9.591322	-0.051960	4.815566
250.928303	7999.993239	9.596327	-0.051995	4.815572
250.835465	7999.983193	9.601331	-0.051978	4.815569
250.684289	7999.993553	9.606336	-0.051950	4.815573
250.827331	8000.008707	9.611341	-0.051976	4.815577
250.934595	7999.976292	9.616346	-0.051996	4.815567
251.062787	7999.990136	9.621351	-0.052020	4.815570
251.106579	7999.978044	9.626355	-0.052029	4.815566
251.114430	7999.972842	9.631360	-0.052030	4.815565
251.199113	7999.999860	9.636365	-0.052046	4.815572
250.906242	7999.976943	9.641370	-0.051992	4.815567
251.108878	8000.001611	9.646375	-0.052029	4.815573
251.084372	7999.989474	9.651379	-0.052025	4.815570
250.866522	7999.984865	9.656384	-0.051984	4.815569
251.192365	8000.002998	9.661389	-0.052045	4.815573
251.351820	7999.984248	9.666394	-0.052075	4.815567
251.444295	8000.008190	9.671399	-0.052092	4.815573
251.232702	7999.989800	9.676403	-0.052053	4.815569
251.378472	7999.981506	9.681408	-0.052080	4.815566
251.438166	7999.999574	9.686413	-0.052092	4.815571
251.212835	7999.961739	9.691418	-0.052050	4.815561
251.183872	7999.995448	9.696423	-0.052044	4.815571
251.159632	8000.034573	9.701427	-0.052040	4.815582
251.116136	8000.006108	9.706432	-0.052032	4.815574
251.158661	8000.004674	9.711437	-0.052040	4.815574
251.211143	8000.009810	9.716442	-0.052050	4.815575
251.187214	8000.012633	9.721447	-0.052046	4.815576
251.111167	7999.980434	9.726451	-0.052031	4.815567
251.253782	7999.990242	9.731456	-0.052058	4.815569
251.120589	8000.005167	9.736461	-0.052033	4.815574
251.166848	7999.984572	9.741466	-0.052042	4.815568
251.104742	8000.003859	9.746471	-0.052031	4.815574
251.221186	7999.983340	9.751475	-0.052052	4.815567
251.118318	7999.979537	9.756480	-0.052033	4.815567
251.133444	8000.021439	9.761485	-0.052036	4.815579
251.118320	7999.978487	9.766490	-0.052034	4.815566
251.205113	8000.001268	9.771495	-0.052050	4.815572
251.069068	7999.992653	9.776499	-0.052025	4.815571
251.022026	7999.997234	9.781504	-0.052016	4.815572
251.384586	8000.026645	9.786509	-0.052084	4.815579
251.326761	7999.968046	9.791514	-0.052073	4.815562
251.328051	7999.995841	9.796519	-0.052073	4.815570
251.151267	7999.987630	9.801523	-0.052040	4.815569
251.139256	7999.975696	9.806528	-0.052038	4.815565
251.371610	8000.005121	9.811533	-0.052082	4.815573
251.249727	7999.977515	9.816538	-0.052059	4.815565
251.226785	7999.982489	9.821543	-0.052055	4.815567
251.205857	7999.981089	9.826547	-0.052051	4.815567
251.187391	7999.957304	9.831552	-0.052048	4.815560
251.337648	7999.999273	9.836557	-0.052076	4.815571
251.328212	7999.962820	9.841562	-0.052074	4.815561
251.279942	7999.996215	9.846567	-0.052065	4.815571
251.460748	7999.992763	9.851571	-0.052099	4.815569
251.391749	7999.990580	9.856576	-0.052086	4.815568
251.472472	8000.018601	9.861581	-0.052102	4.815576
251.464196	7999.972556	9.866586	-0.052100	4.815563
251.444743	8000.013896	9.871591	-0.052097	4.815575
251.244722	8000.005305	9.876595	-0.052059	4.815573
251.308001	7999.987124	9.881600	-0.052071	4.815568
251.357486	8000.017840	9.886605	-0.052081	4.815577
251.333534	7999.997169	9.891610	-0.052076	4.815571
251.410503	8000.019790	9.896615	-0.052091	4.815577
251.293747	8000.001878	9.901619	-0.052069	4.815572
251.352812	7999.990035	9.906624	-0.052080	4.815568
251.405718	8000.016535	9.911629	-0.052090	4.815576
251.423018	7999.991197	9.916634	-0.052093	4.815568
251.644875	8000.025790	9.921639	-0.052135	4.815577
251.480755	8000.007106	9.926643	-0.052104	4.815573
251.444426	7999.989437	9.931648	-0.052098	4.815568
251.779940	8000.051512	9.936653	-0.052160	4.815584
251.599394	8000.025085	9.941658	-0.052127	4.815577
251.465206	8000.025043	9.946663	-0.052102	4.815578
251.644242	7999.995933	9.951667	-0.052135	4.815569
251.520543	8000.007809	9.956672	-0.052112	4.815573
251.430552	7999.999944	9.961677	-0.052096	4.815571
251.564769	7999.983986	9.966682	-0.052121	4.815566
251.601403	8000.003814	9.971687	-0.052128	4.815571
251.609658	8000.002890	9.976691	-0.052129	4.815571
251.551504	7999.993408	9.981696	-0.052119	4.815568
251.627268	8000.023484	9.986701	-0.052133	4.815577
251.579252	7999.984267	9.991706	-0.052124	4.815566
251.631080	8000.019293	9.996711	-0.052134	4.815576
251.377655	8000.021579	10.001715	-0.052087	4.815577
251.484679	7999.990228	10.006720	-0.052107	4.815568
251.363747	8000.027777	10.011725	-0.052084	4.815579
251.321973	7999.994001	10.016730	-0.052077	4.815570
251.346957	7999.989078	10.021735	-0.052081	4.815568
251.386981	7999.998282	10.026739	-0.052089	4.815571
251.344279	7999.990120	10.031744	-0.052081	4.815568
251.512986	8000.007829	10.036749	-0.052113	4.815573
251.546068	7999.979544	10.041754	-0.052119	4.815564
251.501218	8000.008723	10.046759	-0.052111	4.815573
251.491267	8000.007502	10.051763	-0.052109	4.815573
251.577929	7999.992905	10.056768	-0.052125	4.815568
251.510755	8000.000362	10.061773	-0.052113	4.815571
251.342870	7999.986956	10.066778	-0.052082	4.815567
251.488868	8000.003227	10.071783	-0.052109	4.815572
251.644248	7999.996158	10.076787	-0.052138	4.815569
251.509951	7999.997182	10.081792	-0.052113	4.815570
251.599001	8000.003981	10.086797	-0.052130	4.815571
251.495336	7999.988418	10.091802	-0.052110	4.815567
251.421471	7999.984020	10.096807	-0.052097	4.815566
251.632632	7999.990674	10.101811	-0.052136	4.815567
251.626041	7999.987372	10.106816	-0.052135	4.815566
251.616197	8000.000035	10.111821	-0.052133	4.815570
251.520728	7999.970723	10.116826	-0.052116	4.815562
251.726238	8000.005050	10.121831	-0.052154	4.815571
251.649544	7999.993130	10.126835	-0.052140	4.815568
251.550773	7999.978715	10.131840	-0.052122	4.815564
251.461075	8000.014638	10.136845	-0.052105	4.815575
251.655698	7999.993258	10.141850	-0.052141	4.815568
251.381947	8000.009094	10.146855	-0.052091	4.815574
251.640360	8000.011180	10.151859	-0.052139	4.815573
251.651362	7999.988942	10.156864	-0.052141	4.815567
251.743694	8000.016085	10.161869	-0.052158	4.815574
251.369314	7999.987567	10.166874	-0.052089	4.815567
251.610650	8000.018206	10.171879	-0.052134	4.815575
251.731083	8000.010567	10.176883	-0.052156	4.815572
251.680766	8000.000145	10.181888	-0.052147	4.815570
251.686453	8000.021605	10.186893	-0.052148	4.815576
251.781794	7999.990063	10.191898	-0.052166	4.815566
251.688357	8000.016314	10.196903	-0.052149	4.815574
251.643159	8000.002772	10.201907	-0.052140	4.815571
251.636994	8000.019766	10.206912	-0.052139	4.815576
251.672562	8000.037441	10.211917	-0.052146	4.815581
251.509235	8000.001684	10.216922	-0.052116	4.815571
251.465848	8000.024479	10.221927	-0.052108	4.815578
251.526530	8000.007323	10.226931	-0.052119	4.815572
251.748903	8000.014160	10.231936	-0.052161	4.815573
251.753513	8000.029195	10.236941	-0.052162	4.815578
251.796820	8000.006416	10.241946	-0.052170	4.815571
251.760454	8000.014376	10.246951	-0.052163	4.815573
251.551515	8000.016318	10.251955	-0.052124	4.815575
251.633708	8000.013395	10.256960	-0.052140	4.815574
251.765631	8000.053999	10.261965	-0.052164	4.815585
251.596380	7999.996787	10.266970	-0.052133	4.815569
251.721754	8000.022333	10.271975	-0.052156	4.815576
251.581667	8000.000836	10.276979	-0.052130	4.815570
251.600154	7999.980857	10.281984	-0.052134	4.815564
251.714173	8000.024372	10.286989	-0.052155	4.815577
251.734796	7999.985205	10.291994	-0.052159	4.815565
251.570261	8000.010297	10.296999	-0.052129	4.815573
251.656511	7999.993558	10.302003	-0.052145	4.815568
251.720936	7999.992481	10.307008	-0.052157	4.815567
251.946265	8000.015386	10.312013	-0.052199	4.815573
251.833622	7999.997540	10.317018	-0.052178	4.815568
251.816604	8000.001543	10.322023	-0.052175	4.815569
251.950586	8000.022958	10.327027	-0.052200	4.815575
251.723469	8000.001111	10.332032	-0.052158	4.815570
251.629759	8000.030561	10.337037	-0.052141	4.815579
251.821051	8000.010195	10.342042	-0.052176	4.815572
251.630345	8000.004959	10.347047	-0.052141	4.815571
251.665691	8000.003409	10.352051	-0.052148	4.815571
251.630777	8000.015663	10.357056	-0.052141	4.815574
251.807516	8000.029232	10.362061	-0.052174	4.815577
251.701238	7999.981589	10.367066	-0.052154	4.815564
251.557196	8000.012355	10.372071	-0.052128	4.815574
251.868937	8000.002495	10.377075	-0.052186	4.815569
251.586879	7999.989363	10.382080	-0.052133	4.815567
251.754568	8000.013463	10.387085	-0.052165	4.815573
251.878766	7999.993071	10.392090	-0.052188	4.815567
252.069609	8000.018617	10.397095	-0.052224	4.815573
251.939448	8000.035726	10.402099	-0.052200	4.815579
251.689529	8000.001760	10.407104	-0.052153	4.815570
252.021495	8000.022131	10.412109	-0.052215	4.815574
251.838554	8000.006343	10.417114	-0.052181	4.815571
251.993855	7999.999273	10.422119	-0.052210	4.815568
251.911095	7999.991525	10.427123	-0.052195	4.815566
251.726628	8000.000274	10.432128	-0.052161	4.815569
251.775776	8000.014967	10.437133	-0.052170	4.815573
251.758272	7999.993333	10.442138	-0.052167	4.815567
251.777533	8000.028896	10.447143	-0.052170	4.815577
251.832430	8000.018053	10.452147	-0.052181	4.815574
251.688810	7999.995431	10.457152	-0.052154	4.815568
252.154638	8000.019052	10.462157	-0.052241	4.815573
252.050931	8000.015235	10.467162	-0.052222	4.815572
251.925141	8000.003582	10.472167	-0.052198	4.815569
252.042364	8000.007638	10.477171	-0.052220	4.815570
251.922501	8000.001421	10.482176	-0.052198	4.815569
251.946852	7999.990080	10.487181	-0.052203	4.815565
251.880974	7999.971929	10.492186	-0.052190	4.815560
251.876014	8000.003894	10.497191	-0.052190	4.815570
252.052663	8000.013190	10.502195	-0.052223	4.815572
251.850692	7999.985345	10.507200	-0.052185	4.815564
252.116492	8000.039878	10.512205	-0.052235	4.815579
251.767414	7999.997888	10.517210	-0.052170	4.815568
251.780811	8000.032288	10.522215	-0.052172	4.815578
252.048276	8000.015299	10.527219	-0.052222	4.815572
251.990369	8000.010092	10.532224	-0.052212	4.815571
252.119156	8000.041034	10.537229	-0.052236	4.815579
251.979358	8000.012067	10.542234	-0.052210	4.815572
252.056956	8000.012273	10.547239	-0.052224	4.815571
251.929533	8000.010204	10.552243	-0.052201	4.815571
251.926460	7999.989873	10.557248	-0.052200	4.815565
251.999021	8000.014559	10.562253	-0.052214	4.815572
251.904839	8000.014100	10.567258	-0.052197	4.815572
251.759805	8000.021356	10.572263	-0.052170	4.815575
251.810368	8000.006171	10.577267	-0.052179	4.815571
251.912785	8000.011053	10.582272	-0.052198	4.815572
251.829883	8000.013982	10.587277	-0.052183	4.815573
251.790253	7999.973833	10.592282	-0.052176	4.815561
251.844918	7999.984344	10.597287	-0.052186	4.815564
251.883198	8000.005267	10.602291	-0.052193	4.815570
251.853277	7999.998381	10.607296	-0.052188	4.815568
251.904929	8000.008843	10.612301	-0.052197	4.815571
251.955615	7999.980845	10.617306	-0.052207	4.815562
251.864719	8000.007138	10.622311	-0.052190	4.815571
252.057153	8000.019895	10.627315	-0.052226	4.815573
251.894024	7999.994819	10.632320	-0.052196	4.815567
251.896617	8000.009820	10.637325	-0.052196	4.815571
252.044939	7999.990890	10.642330	-0.052224	4.815565
252.074705	8000.041575	10.647335	-0.052230	4.815580
252.183148	8000.024130	10.652339	-0.052250	4.815574
252.046838	8000.001626	10.657344	-0.052225	4.815568
252.058259	8000.046673	10.662349	-0.052227	4.815581
252.110903	8000.028318	10.667354	-0.052237	4.815576
252.072385	8000.044786	10.672359	-0.052230	4.815581
252.028362	8000.039805	10.677363	-0.052222	4.815579
252.031277	8000.007825	10.682368	-0.052222	4.815570
252.039708	8000.031465	10.687373	-0.052224	4.815577
251.862081	8000.009356	10.692378	-0.052191	4.815571
251.910619	8000.011224	10.697383	-0.052200	4.815572
251.996653	8000.019043	10.702387	-0.052216	4.815573
251.796830	7999.998709	10.707392	-0.052179	4.815568
251.750906	8000.027870	10.712397	-0.052171	4.815577
251.967770	7999.991902	10.717402	-0.052211	4.815566
252.137854	7999.990412	10.722407	-0.052243	4.815564
251.973491	8000.003760	10.727411	-0.052213	4.815569
251.897250	7999.997187	10.732416	-0.052198	4.815567
252.126965	8000.031910	10.737421	-0.052241	4.815577
251.975876	8000.017709	10.742426	-0.052213	4.815573
251.999370	8000.004218	10.747431	-0.052218	4.815569
252.152711	8000.010998	10.752435	-0.052246	4.815570
252.016232	7999.991696	10.757440	-0.052221	4.815565
251.953415	8000.034465	10.762445	-0.052210	4.815578
251.937924	8000.013931	10.767450	-0.052207	4.815572
251.822152	8000.006713	10.772455	-0.052185	4.815571
251.834187	8000.011190	10.777459	-0.052188	4.815572
251.962476	7999.989797	10.782464	-0.052212	4.815565
252.045328	8000.008243	10.787469	-0.052227	4.815570
251.826415	8000.000411	10.792474	-0.052187	4.815569
251.828136	8000.002584	10.797479	-0.052187	4.815569
251.841211	8000.009214	10.802483	-0.052189	4.815571
251.929441	7999.988235	10.807488	-0.052206	4.815565
252.027147	8000.006923	10.812493	-0.052224	4.815570
251.946936	7999.989606	10.817498	-0.052209	4.815565
251.974808	8000.019971	10.822503	-0.052215	4.815574
251.894687	8000.014402	10.827507	-0.052200	4.815572
252.013421	8000.005668	10.832512	-0.052222	4.815569
251.969065	7999.998546	10.837517	-0.052214	4.815567
251.943051	7999.990656	10.842522	-0.052209	4.815565
251.964925	8000.005972	10.847527	-0.052213	4.815570
252.082675	8000.008968	10.852531	-0.052235	4.815570
251.929183	7999.992592	10.857536	-0.052207	4.815566
251.794328	8000.010693	10.862541	-0.052182	4.815572
251.902580	8000.002856	10.867546	-0.052202	4.815569
251.941789	8000.013115	10.872551	-0.052210	4.815572
251.904533	8000.028535	10.877555	-0.052203	4.815577
251.936817	7999.973540	10.882560	-0.052209	4.815560
251.949298	7999.992974	10.887565	-0.052211	4.815566
252.133225	7999.995982	10.892570	-0.052246	4.815566
251.985755	8000.010673	10.897575	-0.052218	4.815571
252.279922	8000.029360	10.902579	-0.052273	4.815575
251.916470	7999.992475	10.907584	-0.052206	4.815566
251.982710	8000.011718	10.912589	-0.052218	4.815571
251.993543	8000.015107	10.917594	-0.052220	4.815572
252.100268	8000.009381	10.922599	-0.052240	4.815570
251.957267	8000.019873	10.927603	-0.052214	4.815574
251.847284	7999.997799	10.932608	-0.052193	4.815568
251.967501	8000.037144	10.937613	-0.052216	4.815579
252.014317	8000.006948	10.942618	-0.052225	4.815570
251.826852	8000.011376	10.947623	-0.052190	4.815572
251.946522	8000.034693	10.952627	-0.052212	4.815578
252.038783	7999.999898	10.957632	-0.052229	4.815567
251.829428	8000.008241	10.962637	-0.052191	4.815571
252.039773	8000.008475	10.967642	-0.052230	4.815570
251.966380	8000.011560	10.972647	-0.052216	4.815571
251.934018	8000.028127	10.977651	-0.052210	4.815576
251.972332	8000.002063	10.982656	-0.052218	4.815568
252.139595	8000.005867	10.987661	-0.052249	4.815569
251.871735	7999.970541	10.992666	-0.052199	4.815560
251.916939	8000.019342	10.997671	-0.052208	4.815574
252.149064	8000.031678	11.002675	-0.052251	4.815576
252.020912	7999.983678	11.007680	-0.052227	4.815563
251.923546	8000.024816	11.012685	-0.052209	4.815575
251.910806	8000.019277	11.017690	-0.052207	4.815574
252.053155	8000.022675	11.022695	-0.052233	4.815574
252.173068	8000.013960	11.027699	-0.052256	4.815571
251.826502	7999.958128	11.032704	-0.052191	4.815556
252.009336	8000.018784	11.037709	-0.052226	4.815573
252.027194	7999.998794	11.042714	-0.052229	4.815567
251.942349	8000.025185	11.047719	-0.052213	4.815575
252.174329	8000.019365	11.052723	-0.052257	4.815572
252.186311	8000.001415	11.057728	-0.052259	4.815567
252.127443	8000.009008	11.062733	-0.052248	4.815570
252.207196	7999.999638	11.067738	-0.052263	4.815567
252.231252	7999.997903	11.072743	-0.052268	4.815566
252.125985	8000.005807	11.077747	-0.052248	4.815569
252.041424	8000.010845	11.082752	-0.052232	4.815571
252.201853	8000.020945	11.087757	-0.052262	4.815573
252.290708	8000.023470	11.092762	-0.052279	4.815573
252.009308	8000.024231	11.097767	-0.052227	4.815575
252.079234	8000.045670	11.102771	-0.052240	4.815581
252.173958	8000.010915	11.107776	-0.052258	4.815570
252.263820	8000.047630	11.112781	-0.052275	4.815580
251.918365	8000.040938	11.117786	-0.052210	4.815580
251.959478	8000.023463	11.122791	-0.052218	4.815575
252.356831	8000.029951	11.127795	-0.052292	4.815575
252.064092	7999.999557	11.132800	-0.052238	4.815567
252.210868	8000.010502	11.137805	-0.052265	4.815570
252.190396	8000.013381	11.142810	-0.052261	4.815571
252.204942	8000.011492	11.147815	-0.052264	4.815570
252.061611	8000.018775	11.152819	-0.052238	4.815573
252.046461	7999.998247	11.157824	-0.052235	4.815567
251.942481	8000.027530	11.162829	-0.052216	4.815576
252.197121	7999.999653	11.167834	-0.052263	4.815567
252.378616	8000.009029	11.172839	-0.052297	4.815568
252.233013	8000.021614	11.177843	-0.052270	4.815573
252.025021	7999.977652	11.182848	-0.052231	4.815561
252.099535	7999.998098	11.187853	-0.052245	4.815567
252.147560	7999.989279	11.192858	-0.052255	4.815564
252.082030	8000.021324	11.197863	-0.052242	4.815573
252.151616	8000.035283	11.202867	-0.052255	4.815577
252.083982	8000.009627	11.207872	-0.052243	4.815570
252.147737	8000.042713	11.212877	-0.052255	4.815579
252.058791	8000.043407	11.217882	-0.052239	4.815580
252.188056	8000.027370	11.222887	-0.052263	4.815575
252.323205	8000.037058	11.227891	-0.052288	4.815577
252.180678	8000.009113	11.232896	-0.052262	4.815569
252.270761	8000.027677	11.237901	-0.052278	4.815574
252.345695	8000.055606	11.242906	-0.052292	4.815582
252.136478	8000.039388	11.247911	-0.052254	4.815578
252.077022	8000.035224	11.252915	-0.052243	4.815577
251.978644	7999.998389	11.257920	-0.052224	4.815567
251.927904	8000.011453	11.262925	-0.052215	4.815571
252.155213	7999.985267	11.267930	-0.052257	4.815562
252.136538	8000.013805	11.272935	-0.052254	4.815571
252.356463	8000.038758	11.277939	-0.052295	4.815577
252.246189	8000.025222	11.282944	-0.052275	4.815574
252.337181	8000.038461	11.287949	-0.052292	4.815577
252.522957	8000.037228	11.292954	-0.052326	4.815576
252.232164	8000.012205	11.297959	-0.052272	4.815570
252.183384	8000.011419	11.302963	-0.052263	4.815570
252.332526	8000.005316	11.307968	-0.052291	4.815567
252.414877	8000.054724	11.312973	-0.052307	4.815582
252.240727	7999.997430	11.317978	-0.052274	4.815566
252.243252	8000.016702	11.322983	-0.052275	4.815571
252.252514	8000.035017	11.327987	-0.052277	4.815577
252.156038	8000.001416	11.332992	-0.052259	4.815567
252.237854	8000.046542	11.337997	-0.052274	4.815580
252.190897	8000.011613	11.343002	-0.052266	4.815570
252.103788	8000.026220	11.348007	-0.052250	4.815575
252.089813	8000.029205	11.353011	-0.052247	4.815576
252.110122	8000.012459	11.358016	-0.052251	4.815571
252.419843	8000.048487	11.363021	-0.052309	4.815580
252.329875	8000.034214	11.368026	-0.052292	4.815576
252.306375	8000.048791	11.373031	-0.052288	4.815580
252.215550	8000.032368	11.378035	-0.052271	4.815576
251.971425	8000.004903	11.383040	-0.052226	4.815569
251.981686	8000.037116	11.388045	-0.052228	4.815578
252.212370	7999.997102	11.393050	-0.052271	4.815566
252.343403	8000.022742	11.398055	-0.052295	4.815572
252.330715	8000.032155	11.403059	-0.052293	4.815575
252.186239	8000.014858	11.408064	-0.052266	4.815571
252.214272	8000.044157	11.413069	-0.052271	4.815579
252.214320	8000.052710	11.418074	-0.052272	4.815582
252.116470	8000.029765	11.423079	-0.052253	4.815576
252.272150	8000.064350	11.428083	-0.052283	4.815585
252.138302	8000.019460	11.433088	-0.052258	4.815572
252.074048	8000.053662	11.438093	-0.052246	4.815583
252.207733	8000.047308	11.443098	-0.052271	4.815580
252.217048	8000.043197	11.448103	-0.052273	4.815579
252.233506	8000.048814	11.453107	-0.052276	4.815581
252.061410	8000.018252	11.458112	-0.052244	4.815572
252.271056	8000.053716	11.463117	-0.052283	4.815582
252.345162	8000.041050	11.468122	-0.052297	4.815578
252.266930	8000.034444	11.473127	-0.052283	4.815576
252.441890	8000.054393	11.478131	-0.052315	4.815581
252.526947	8000.019480	11.483136	-0.052331	4.815571
252.398024	8000.034473	11.488141	-0.052307	4.815576
252.356396	8000.018853	11.493146	-0.052300	4.815571
252.294414	8000.017851	11.498151	-0.052288	4.815571
252.464554	8000.045196	11.503155	-0.052320	4.815578
252.179236	8000.035213	11.508160	-0.052267	4.815577
252.339351	8000.067734	11.513165	-0.052297	4.815586
252.303767	8000.046873	11.518170	-0.052290	4.815580
252.228368	8000.024294	11.523175	-0.052276	4.815573
252.408231	8000.043255	11.528179	-0.052310	4.815578
252.205953	8000.028218	11.533184	-0.052272	4.815575
252.221075	8000.041289	11.538189	-0.052275	4.815578
252.146062	8000.028328	11.543194	-0.052261	4.815575
252.318215	8000.026872	11.548199	-0.052294	4.815574
252.282194	8000.018818	11.553203	-0.052287	4.815572
252.380753	8000.003348	11.558208	-0.052305	4.815567
252.479814	8000.009244	11.563213	-0.052324	4.815568
252.403704	8000.017623	11.568218	-0.052310	4.815571
252.308017	8000.035294	11.573223	-0.052292	4.815576
252.262221	8000.035624	11.578227	-0.052284	4.815577
252.132946	8000.008963	11.583232	-0.052260	4.815569
252.315489	8000.033307	11.588237	-0.052294	4.815576
252.251421	7999.991691	11.593242	-0.052282	4.815564
252.287894	7999.990159	11.598247	-0.052289	4.815563
252.300008	8000.039489	11.603251	-0.052291	4.815577
252.400127	8000.049674	11.608256	-0.052310	4.815580
252.479249	8000.063788	11.613261	-0.052325	4.815584
252.522383	8000.045278	11.618266	-0.052333	4.815578
252.328013	8000.038914	11.623271	-0.052297	4.815577
252.431531	8000.051290	11.628275	-0.052316	4.815580
252.366408	8000.034218	11.633280	-0.052304	4.815576
252.255228	8000.032414	11.638285	-0.052284	4.815576
252.363761	8000.026717	11.643290	-0.052304	4.815573
252.189461	7999.997187	11.648295	-0.052272	4.815566
252.380922	8000.033423	11.653299	-0.052307	4.815575
252.411276	8000.028587	11.658304	-0.052313	4.815574
252.281541	8000.058518	11.663309	-0.052289	4.815583
252.467710	8000.057291	11.668314	-0.052324	4.815582
252.336807	8000.046622	11.673319	-0.052300	4.815579
252.419499	8000.096035	11.678323	-0.052315	4.815593
252.298221	8000.007566	11.683328	-0.052293	4.815568
252.341198	8000.033906	11.688333	-0.052301	4.815576
252.339154	8000.026406	11.693338	-0.052300	4.815573
252.288069	8000.003156	11.698343	-0.052291	4.815567
252.316171	8000.043136	11.703347	-0.052296	4.815578
252.035624	8000.017212	11.708352	-0.052244	4.815572
252.313905	8000.053796	11.713357	-0.052296	4.815582
252.373607	8000.024877	11.718362	-0.052307	4.815573
252.061639	8000.009120	11.723367	-0.052249	4.815570
252.349979	8000.038392	11.728371	-0.052303	4.815577
252.325256	8000.005961	11.733376	-0.052299	4.815567
252.218095	8000.023445	11.738381	-0.052279	4.815573
252.283486	8000.038403	11.743386	-0.052291	4.815577
252.196874	8000.015642	11.748391	-0.052275	4.815571
252.373395	8000.046295	11.753395	-0.052308	4.815579
252.273035	8000.029716	11.758400	-0.052289	4.815575
252.431420	8000.054734	11.763405	-0.052319	4.815581
252.549556	8000.052398	11.768410	-0.052341	4.815580
252.333038	8000.041401	11.773415	-0.052301	4.815578
252.601663	8000.044722	11.778419	-0.052351	4.815577
252.294808	8000.035456	11.783424	-0.052294	4.815576
252.179178	8000.010086	11.788429	-0.052273	4.815569
252.331508	8000.036072	11.793434	-0.052301	4.815576
252.608056	8000.028844	11.798439	-0.052353	4.815573
252.571320	8000.067767	11.803443	-0.052346	4.815584
252.320933	8000.017772	11.808448	-0.052299	4.815571
252.355411	8000.024751	11.813453	-0.052306	4.815573
252.587657	8000.025343	11.818458	-0.052349	4.815572
252.537111	8000.012781	11.823463	-0.052340	4.815568
252.448442	8000.061536	11.828467	-0.052324	4.815583
252.398060	8000.024414	11.833472	-0.052314	4.815572
252.380474	8000.071125	11.838477	-0.052311	4.815586
252.523392	8000.069193	11.843482	-0.052338	4.815585
252.294955	8000.035575	11.848487	-0.052295	4.815576
252.293165	8000.075067	11.853491	-0.052295	4.815588
252.163808	8000.034522	11.858496	-0.052271	4.815577
252.132603	8000.079942	11.863501	-0.052266	4.815590
252.392116	8000.029720	11.868506	-0.052314	4.815574
252.277111	8000.042804	11.873511	-0.052293	4.815578
252.437214	8000.071054	11.878515	-0.052323	4.815586
252.396795	8000.039434	11.883520	-0.052315	4.815577
252.588922	8000.065003	11.888525	-0.052351	4.815583
252.478243	8000.024762	11.893530	-0.052330	4.815572
252.476121	8000.009786	11.898535	-0.052330	4.815568
252.627553	8000.082746	11.903539	-0.052359	4.815588
252.467396	8000.039563	11.908544	-0.052329	4.815577
252.483218	8000.069731	11.913549	-0.052332	4.815585
252.684177	8000.079425	11.918554	-0.052369	4.815587
252.313341	8000.056300	11.923559	-0.052300	4.815582
252.323478	8000.071425	11.928563	-0.052302	4.815587
252.358604	8000.050648	11.933568	-0.052309	4.815580
252.477061	8000.068608	11.938573	-0.052331	4.815585
252.332915	8000.069470	11.943578	-0.052304	4.815586
252.287518	8000.045245	11.948583	-0.052296	4.815579
252.441630	8000.056310	11.953587	-0.052325	4.815582
252.440491	8000.074455	11.958592	-0.052325	4.815587
252.279945	8000.082525	11.963597	-0.052295	4.815590
252.443218	8000.073449	11.968602	-0.052326	4.815587
252.348497	8000.017450	11.973607	-0.052308	4.815571
252.428591	8000.037988	11.978611	-0.052323	4.815576
252.389841	8000.038433	11.983616	-0.052316	4.815577
252.397965	8000.037506	11.988621	-0.052317	4.815576
252.448921	8000.029803	11.993626	-0.052327	4.815574
252.288618	8000.020790	11.998631	-0.052297	4.815572
252.532604	8000.042933	12.003635	-0.052343	4.815577
252.598836	8000.041886	12.008640	-0.052355	4.815577
252.286891	8000.049623	12.013645	-0.052297	4.815580
252.531729	8000.060032	12.018650	-0.052343	4.815582
252.433082	8000.025327	12.023655	-0.052325	4.815572
252.362691	8000.046614	12.028659	-0.052312	4.815579
252.320371	8000.041661	12.033664	-0.052304	4.815578
252.325187	8000.035341	12.038669	-0.052305	4.815576
252.352704	8000.055021	12.043674	-0.052310	4.815582
252.390737	8000.019342	12.048679	-0.052317	4.815571
252.559646	8000.061618	12.053683	-0.052349	4.815582
252.696430	8000.015802	12.058688	-0.052374	4.815568
252.613808	8000.043297	12.063693	-0.052359	4.815577
252.655288	8000.033303	12.068698	-0.052367	4.815574
252.551552	8000.030552	12.073703	-0.052348	4.815573
252.458279	8000.039719	12.078707	-0.052331	4.815577
252.374452	8000.007392	12.083712	-0.052315	4.815567
252.457825	8000.041866	12.088717	-0.052331	4.815577
252.543734	8000.025121	12.093722	-0.052347	4.815572
252.352878	8000.010271	12.098727	-0.052311	4.815568
252.427430	8000.057416	12.103731	-0.052325	4.815582
252.318462	8000.037493	12.108736	-0.052305	4.815577
252.280472	8000.060377	12.113741	-0.052298	4.815583
252.446548	8000.043872	12.118746	-0.052329	4.815578
252.574990	8000.038500	12.123751	-0.052353	4.815576
252.398269	8000.027084	12.128755	-0.052320	4.815573
252.333656	7999.999341	12.133760	-0.052308	4.815565
252.382235	8000.041791	12.138765	-0.052318	4.815577
252.372433	8000.042708	12.143770	-0.052316	4.815578
252.405976	8000.040060	12.148775	-0.052322	4.815577
252.616403	8000.069131	12.153779	-0.052362	4.815584
252.518209	8000.024822	12.158784	-0.052343	4.815572
252.306803	8000.050217	12.163789	-0.052304	4.815580
252.328804	8000.044177	12.168794	-0.052308	4.815578
252.402091	8000.026159	12.173799	-0.052322	4.815573
252.567059	8000.041673	12.178803	-0.052353	4.815577
252.527074	8000.043166	12.183808	-0.052346	4.815577
252.624286	8000.053304	12.188813	-0.052364	4.815580
252.589230	8000.031383	12.193818	-0.052357	4.815573
252.455723	8000.038825	12.198823	-0.052333	4.815576
252.587713	8000.052734	12.203827	-0.052357	4.815580
252.347862	8000.016794	12.208832	-0.052313	4.815570
252.275692	8000.044460	12.213837	-0.052299	4.815579
252.424699	8000.039423	12.218842	-0.052327	4.815577
252.598013	8000.020901	12.223847	-0.052360	4.815570
252.588121	8000.047446	12.228851	-0.052358	4.815578
252.255349	8000.009991	12.233856	-0.052296	4.815569
252.365147	8000.024605	12.238861	-0.052316	4.815572
252.496609	8000.017147	12.243866	-0.052341	4.815570
252.354476	7999.996684	12.248871	-0.052315	4.815564
252.609048	8000.040357	12.253875	-0.052362	4.815576
252.495877	7999.993668	12.258880	-0.052341	4.815563
252.562993	8000.017198	12.263885	-0.052354	4.815569
252.566528	8000.009789	12.268890	-0.052355	4.815567
252.552307	8000.008498	12.273895	-0.052352	4.815567
252.414529	8000.023347	12.278899	-0.052326	4.815572
252.482236	8000.005237	12.283904	-0.052339	4.815566
252.525471	8000.032649	12.288909	-0.052347	4.815574
252.565462	8000.029039	12.293914	-0.052355	4.815573
252.246994	8000.006768	12.298919	-0.052296	4.815568
252.467196	8000.027454	12.303923	-0.052337	4.815573
252.564183	7999.997008	12.308928	-0.052355	4.815563
252.487785	8000.035283	12.313933	-0.052341	4.815575
252.508461	8000.033494	12.318938	-0.052345	4.815574
252.540623	8000.013737	12.323943	-0.052351	4.815568
252.592645	8000.038088	12.328947	-0.052361	4.815575
252.616757	8000.020336	12.333952	-0.052365	4.815570
252.498488	8000.037639	12.338957	-0.052343	4.815576
252.491104	8000.028984	12.343962	-0.052342	4.815573
252.339573	8000.028658	12.348967	-0.052314	4.815574
252.547339	8000.047006	12.353971	-0.052353	4.815578
252.635397	8000.007870	12.358976	-0.052369	4.815566
252.402754	8000.030783	12.363981	-0.052326	4.815574
252.251099	8000.013368	12.368986	-0.052298	4.815570
252.333458	7999.993362	12.373991	-0.052313	4.815563
252.498602	8000.040916	12.378995	-0.052344	4.815577
252.589246	8000.033860	12.384000	-0.052361	4.815574
252.671533	8000.019192	12.389005	-0.052377	4.815569
252.394070	8000.017880	12.394010	-0.052325	4.815570
252.411277	7999.996812	12.399015	-0.052328	4.815564
252.570246	8000.042129	12.404019	-0.052358	4.815577
252.715522	8000.010334	12.409024	-0.052385	4.815567
252.708325	8000.030516	12.414029	-0.052384	4.815572
252.444608	8000.031564	12.419034	-0.052335	4.815574
252.651498	8000.045626	12.424039	-0.052374	4.815577
252.762947	8000.082694	12.429043	-0.052394	4.815587
252.534854	8000.055489	12.434048	-0.052352	4.815581
252.453313	8000.043489	12.439053	-0.052337	4.815577
252.628259	8000.030332	12.444058	-0.052370	4.815573
252.521944	8000.015793	12.449063	-0.052350	4.815569
252.479119	8000.050344	12.454067	-0.052342	4.815579
252.693965	8000.014344	12.459072	-0.052382	4.815568
252.651511	8000.040359	12.464077	-0.052374	4.815576
252.575940	8000.036999	12.469082	-0.052360	4.815575
252.493527	8000.012170	12.474087	-0.052345	4.815568
252.622576	8000.043118	12.479091	-0.052369	4.815577
252.625199	8000.019675	12.484096	-0.052370	4.815570
252.443317	8000.008175	12.489101	-0.052336	4.815567
252.593649	8000.013839	12.494106	-0.052364	4.815568
252.542399	7999.992722	12.499111	-0.052355	4.815562
252.471139	8000.030014	12.504115	-0.052342	4.815573
252.545186	8000.004532	12.509120	-0.052356	4.815566
252.608267	8000.027996	12.514125	-0.052367	4.815572
252.751859	8000.013260	12.519130	-0.052394	4.815567
252.551010	8000.016401	12.524135	-0.052357	4.815569
252.698812	8000.056198	12.529139	-0.052385	4.815580
252.575065	8000.014676	12.534144	-0.052362	4.815568
252.693055	8000.046511	12.539149	-0.052384	4.815577
252.692897	8000.053993	12.544154	-0.052384	4.815579
252.657549	8000.003233	12.549159	-0.052377	4.815565
252.419183	8000.036732	12.554163	-0.052333	4.815576
252.393367	8000.017097	12.559168	-0.052328	4.815570
252.670076	8000.023755	12.564173	-0.052380	4.815571
252.584158	8000.050128	12.569178	-0.052364	4.815579
252.528739	8000.022536	12.574183	-0.052354	4.815571
252.731281	8000.058953	12.579187	-0.052392	4.815581
252.670478	8000.035544	12.584192	-0.052380	4.815574
252.483244	8000.033568	12.589197	-0.052346	4.815574
252.702092	8000.029670	12.594202	-0.052387	4.815572
252.583247	8000.032013	12.599207	-0.052364	4.815573
252.501202	8000.029616	12.604211	-0.052349	4.815573
252.557951	8000.013464	12.609216	-0.052360	4.815568
252.720030	8000.023591	12.614221	-0.052390	4.815570
252.608868	8000.031399	12.619226	-0.052370	4.815573
252.543121	8000.005773	12.624231	-0.052358	4.815566
252.620738	8000.030542	12.629235	-0.052372	4.815573
252.442647	7999.998813	12.634240	-0.052339	4.815564
252.493449	8000.019941	12.639245	-0.052349	4.815570
252.478910	8000.034664	12.644250	-0.052346	4.815575
252.595559	8000.030167	12.649255	-0.052368	4.815573
252.468115	8000.041981	12.654259	-0.052344	4.815577
252.374696	8000.025516	12.659264	-0.052327	4.815572
252.500182	8000.033979	12.664269	-0.052350	4.815574
252.638037	8000.056526	12.669274	-0.052376	4.815580
252.324171	8000.036466	12.674279	-0.052318	4.815576
252.536301	8000.028187	12.679283	-0.052357	4.815572
252.614932	8000.040158	12.684288	-0.052372	4.815576
252.277531	8000.037868	12.689293	-0.052309	4.815577
252.578712	8000.051332	12.694298	-0.052366	4.815579
252.782395	8000.053595	12.699303	-0.052404	4.815579
252.563786	8000.056446	12.704307	-0.052363	4.815581
252.453915	8000.009811	12.709312	-0.052343	4.815567
252.523819	8000.030182	12.714317	-0.052356	4.815573
252.683589	8000.056291	12.719322	-0.052386	4.815580
252.511999	8000.008649	12.724327	-0.052354	4.815567
252.776410	8000.048212	12.729331	-0.052403	4.815577
252.872080	8000.034830	12.734336	-0.052421	4.815573
252.691179	8000.042568	12.739341	-0.052387	4.815576
252.667343	8000.048596	12.744346	-0.052383	4.815578
252.706776	8000.039636	12.749351	-0.052391	4.815575
252.563561	8000.051193	12.754355	-0.052364	4.815579
252.401184	8000.028263	12.759360	-0.052334	4.815573
252.524017	8000.031343	12.764365	-0.052357	4.815573
252.708947	8000.032232	12.769370	-0.052391	4.815573
252.481393	8000.030666	12.774375	-0.052349	4.815573
252.615247	8000.043537	12.779379	-0.052374	4.815577
252.812725	8000.022205	12.784384	-0.052411	4.815569
252.606496	8000.020986	12.789389	-0.052373	4.815570
252.595619	8000.021886	12.794394	-0.052371	4.815570
252.569137	8000.020395	12.799399	-0.052366	4.815570
252.653202	8000.044201	12.804403	-0.052382	4.815577
252.720247	8000.043168	12.809408	-0.052394	4.815576
252.706122	8000.036539	12.814413	-0.052392	4.815574
252.746363	8000.036136	12.819418	-0.052399	4.815574
252.654565	8000.013290	12.824423	-0.052382	4.815567
252.790769	8000.043286	12.829427	-0.052408	4.815576
252.851968	8000.028274	12.834432	-0.052419	4.815571
252.851249	8000.038951	12.839437	-0.052419	4.815574
252.749937	8000.046919	12.844442	-0.052401	4.815577
252.702030	8000.006633	12.849447	-0.052392	4.815565
252.767686	8000.035479	12.854451	-0.052404	4.815573
252.618472	8000.009560	12.859456	-0.052376	4.815567
252.582697	8000.028208	12.864461	-0.052370	4.815572
252.897006	8000.040819	12.869466	-0.052428	4.815574
252.770261	8000.002451	12.874471	-0.052405	4.815564
252.759101	8000.039656	12.879475	-0.052403	4.815575
252.810854	8000.021286	12.884480	-0.052413	4.815569
252.768519	8000.043031	12.889485	-0.052405	4.815576
252.770973	8000.052691	12.894490	-0.052406	4.815578
252.591404	8000.001715	12.899495	-0.052372	4.815564
252.900526	8000.059094	12.904499	-0.052430	4.815580
252.713233	8000.036826	12.909504	-0.052395	4.815574
252.617793	8000.036346	12.914509	-0.052377	4.815574
252.735472	8000.037206	12.919514	-0.052399	4.815574
252.737152	8000.013748	12.924519	-0.052400	4.815567
252.718754	8000.045495	12.929523	-0.052396	4.815577
252.641626	8000.030363	12.934528	-0.052382	4.815572
252.617153	8000.038516	12.939533	-0.052378	4.815575
252.601423	8000.033997	12.944538	-0.052375	4.815574
252.797869	8000.008376	12.949543	-0.052412	4.815565
252.887192	8000.049355	12.954547	-0.052428	4.815577
252.669877	8000.011646	12.959552	-0.052388	4.815567
252.735847	8000.033022	12.964557	-0.052400	4.815573
252.941278	8000.037449	12.969562	-0.052439	4.815573
252.882525	8000.026889	12.974567	-0.052428	4.815570
252.745208	8000.044948	12.979571	-0.052402	4.815576
252.675326	8000.033138	12.984576	-0.052390	4.815573
252.813906	8000.050358	12.989581	-0.052415	4.815577
252.720888	8000.031764	12.994586	-0.052398	4.815572
252.680679	8000.015098	12.999591	-0.052391	4.815568
252.685098	8000.047217	13.004595	-0.052392	4.815577
252.489324	8000.030150	13.009600	-0.052355	4.815573
252.387010	8000.017811	13.014605	-0.052336	4.815570
252.603361	8000.023484	13.019610	-0.052377	4.815571
252.354109	7999.978848	13.024615	-0.052331	4.815559
252.515357	8000.024203	13.029619	-0.052361	4.815571
252.467944	7999.999944	13.034624	-0.052352	4.815564
252.519985	8000.033907	13.039629	-0.052362	4.815574
252.462179	8000.037245	13.044634	-0.052351	4.815575
252.526929	8000.025495	13.049639	-0.052363	4.815572
252.739565	8000.052466	13.054643	-0.052403	4.815578
252.627928	8000.023957	13.059648	-0.052382	4.815571
252.539307	8000.013977	13.064653	-0.052366	4.815568
252.585420	8000.020078	13.069658	-0.052375	4.815570
252.665798	8000.011786	13.074663	-0.052390	4.815567
252.528669	8000.028781	13.079667	-0.052364	4.815572
252.636808	8000.030554	13.084672	-0.052384	4.815572
252.622747	8000.028198	13.089677	-0.052382	4.815572
252.666604	8000.042805	13.094682	-0.052390	4.815576
252.540488	8000.011923	13.099687	-0.052367	4.815567
252.562257	8000.049664	13.104691	-0.052371	4.815578
252.560328	8000.038963	13.109696	-0.052371	4.815575
252.620483	8000.030342	13.114701	-0.052382	4.815572
252.680492	8000.033465	13.119706	-0.052393	4.815573
252.408328	8000.022628	13.124711	-0.052343	4.815571
252.303993	8000.041226	13.129715	-0.052323	4.815577
252.462857	8000.019264	13.134720	-0.052353	4.815570
252.616374	8000.013233	13.139725	-0.052382	4.815567
252.512091	8000.024356	13.144730	-0.052362	4.815571
252.442582	8000.017892	13.149735	-0.052350	4.815570
252.523421	8000.035238	13.154739	-0.052365	4.815574
252.473515	8000.012007	13.159744	-0.052356	4.815568
252.431046	8000.019867	13.164749	-0.052348	4.815570
252.583612	8000.030907	13.169754	-0.052376	4.815573
252.617689	8000.010113	13.174759	-0.052383	4.815567
252.421272	8000.027210	13.179763	-0.052346	4.815572
252.715694	8000.025613	13.184768	-0.052401	4.815571
252.703927	8000.019022	13.189773	-0.052399	4.815569
252.804301	8000.038823	13.194778	-0.052418	4.815574
252.366660	8000.000725	13.199783	-0.052336	4.815565
252.658885	8000.050352	13.204787	-0.052391	4.815578
252.678244	8000.035726	13.209792	-0.052395	4.815574
252.432992	8000.023192	13.214797	-0.052349	4.815571
252.464749	8000.066435	13.219802	-0.052355	4.815584
252.541988	8000.019648	13.224807	-0.052370	4.815570
252.714568	8000.060917	13.229811	-0.052402	4.815581
252.637889	8000.037249	13.234816	-0.052388	4.815574
252.565218	8000.021122	13.239821	-0.052374	4.815570
252.568110	8000.040400	13.244826	-0.052375	4.815576
252.390611	7999.989459	13.249831	-0.052342	4.815562
252.660097	8000.031239	13.254835	-0.052392	4.815572
252.571944	7999.992434	13.259840	-0.052376	4.815562
252.487511	8000.020967	13.264845	-0.052360	4.815570
252.576048	8000.039507	13.269850	-0.052377	4.815575
252.467169	8000.008906	13.274855	-0.052357	4.815567
252.403918	8000.040989	13.279859	-0.052345	4.815577
252.506381	8000.003156	13.284864	-0.052364	4.815565
252.673905	8000.021916	13.289869	-0.052396	4.815570
252.665536	8000.047419	13.294874	-0.052394	4.815577
252.465777	8000.008929	13.299879	-0.052357	4.815567
252.367430	8000.015877	13.304883	-0.052339	4.815569
252.585944	8000.017314	13.309888	-0.052380	4.815569
252.510399	8000.043856	13.314893	-0.052366	4.815577
252.490006	8000.076638	13.319898	-0.052362	4.815587
252.555172	8000.013635	13.324903	-0.052374	4.815568
252.757751	8000.031899	13.329907	-0.052412	4.815572
252.602736	8000.009089	13.334912	-0.052383	4.815566
252.602601	8000.002688	13.339917	-0.052383	4.815564
252.709651	8000.023666	13.344922	-0.052403	4.815570
252.569453	8000.026728	13.349927	-0.052377	4.815572
252.661223	8000.057067	13.354931	-0.052395	4.815580
252.711719	8000.046153	13.359936	-0.052404	4.815577
252.506335	8000.027861	13.364941	-0.052366	4.815572
252.541206	8000.019896	13.369946	-0.052372	4.815570
252.623074	8000.012697	13.374951	-0.052388	4.815567
252.429703	8000.057608	13.379955	-0.052352	4.815581
252.555638	8000.050060	13.384960	-0.052375	4.815578
252.479808	8000.008251	13.389965	-0.052361	4.815567
252.694760	8000.069433	13.394970	-0.052402	4.815583
252.401123	8000.026208	13.399975	-0.052347	4.815572
252.458684	8000.047446	13.404979	-0.052358	4.815578
252.486777	8000.007333	13.409984	-0.052363	4.815566
252.654840	8000.014354	13.414989	-0.052395	4.815567
252.715066	8000.052723	13.419994	-0.052406	4.815578
252.644746	8000.023819	13.424999	-0.052393	4.815570
252.754454	8000.041636	13.430003	-0.052413	4.815575
252.609977	8000.009387	13.435008	-0.052387	4.815566
252.550955	8000.023384	13.440013	-0.052376	4.815571
252.649683	8000.057041	13.445018	-0.052394	4.815580
252.564696	8000.019355	13.450023	-0.052378	4.815569
252.579750	8000.029220	13.455027	-0.052381	4.815572
252.594188	8000.035872	13.460032	-0.052384	4.815574
252.557467	8000.018196	13.465037	-0.052377	4.815569
252.434453	8000.029014	13.470042	-0.052355	4.815573
252.483253	8000.015936	13.475047	-0.052364	4.815569
252.651305	8000.041111	13.480051	-0.052395	4.815575
252.508419	8000.033451	13.485056	-0.052369	4.815574
252.380320	8000.015352	13.490061	-0.052345	4.815569
252.558708	8000.058851	13.495066	-0.052378	4.815581
252.335248	8000.002888	13.500071	-0.052337	4.815566
252.255123	8000.028288	13.505075	-0.052322	4.815573
252.524934	8000.014542	13.510080	-0.052372	4.815568
252.562126	8000.024769	13.515085	-0.052379	4.815571
252.472869	8000.046816	13.520090	-0.052363	4.815578
252.466161	8000.016815	13.525095	-0.052362	4.815569
252.555395	8000.031094	13.530099	-0.052378	4.815573
252.500751	8000.021668	13.535104	-0.052368	4.815570
252.477955	8000.014898	13.540109	-0.052364	4.815568
252.622767	8000.033287	13.545114	-0.052391	4.815573
252.615158	8000.013950	13.550119	-0.052390	4.815567
252.626785	8000.045118	13.555123	-0.052392	4.815577
252.667905	8000.040458	13.560128	-0.052400	4.815575
252.468943	8000.021203	13.565133	-0.052363	4.815570
252.470518	8000.042596	13.570138	-0.052363	4.815577
252.584230	8000.009219	13.575143	-0.052385	4.815566
252.620314	8000.036514	13.580147	-0.052391	4.815574
252.467507	8000.034031	13.585152	-0.052363	4.815574
252.425329	8000.018401	13.590157	-0.052355	4.815570
252.788170	8000.064909	13.595162	-0.052423	4.815582
252.835473	8000.022973	13.600167	-0.052432	4.815569
252.631432	8000.047419	13.605171	-0.052394	4.815577
252.620204	8000.036566	13.610176	-0.052392	4.815574
252.609957	8000.037476	13.615181	-0.052390	4.815574
252.456278	8000.044590	13.620186	-0.052362	4.815577
252.372017	8000.016527	13.625191	-0.052346	4.815569
252.548617	8000.024755	13.630195	-0.052379	4.815571
252.564431	8000.027158	13.635200	-0.052382	4.815572
252.528305	8000.004152	13.640205	-0.052376	4.815565
252.612317	8000.027957	13.645210	-0.052391	4.815572
252.489412	8000.015282	13.650215	-0.052369	4.815568
252.457508	8000.028654	13.655219	-0.052363	4.815572
252.671482	8000.024677	13.660224	-0.052403	4.815570
252.737408	8000.014014	13.665229	-0.052415	4.815567
252.690743	8000.037824	13.670234	-0.052406	4.815574
252.438949	7999.993146	13.675239	-0.052360	4.815562
252.710303	8000.017871	13.680243	-0.052410	4.815568
252.706987	8000.066950	13.685248	-0.052410	4.815582
252.502243	8000.037990	13.690253	-0.052372	4.815575
252.793068	8000.060897	13.695258	-0.052426	4.815580
252.679829	8000.003527	13.700263	-0.052405	4.815564
252.623973	8000.018644	13.705267	-0.052395	4.815569
252.531902	8000.013947	13.710272	-0.052378	4.815568
252.495139	8000.008017	13.715277	-0.052371	4.815566
252.630711	8000.031596	13.720282	-0.052396	4.815572
252.561060	7999.990956	13.725287	-0.052383	4.815561
252.655402	8000.020269	13.730291	-0.052401	4.815569
252.690681	8000.000563	13.735296	-0.052408	4.815563
252.617681	8000.018604	13.740301	-0.052394	4.815569
252.727475	8000.056713	13.745306	-0.052415	4.815579
252.767158	8000.028535	13.750311	-0.052422	4.815571
252.620949	8000.034703	13.755315	-0.052395	4.815573
252.553675	8000.026139	13.760320	-0.052383	4.815571
252.638454	7999.995494	13.765325	-0.052399	4.815562
252.633158	8000.026386	13.770330	-0.052398	4.815571
252.610643	7999.999330	13.775335	-0.052394	4.815563
252.702522	8000.021128	13.780339	-0.052411	4.815569
252.791905	8000.022594	13.785344	-0.052428	4.815569
252.638814	7999.996612	13.790349	-0.052399	4.815562
252.591367	8000.041768	13.795354	-0.052391	4.815576
252.562130	7999.996448	13.800359	-0.052385	4.815562
252.533380	8000.051519	13.805363	-0.052380	4.815579
252.535513	8000.055835	13.810368	-0.052380	4.815580
252.619263	8000.049734	13.815373	-0.052396	4.815578
252.707022	8000.058650	13.820378	-0.052413	4.815580
252.570045	8000.024387	13.825383	-0.052387	4.815571
252.682915	8000.029441	13.830387	-0.052408	4.815572
252.811361	8000.023002	13.835392	-0.052432	4.815569
252.578130	8000.011731	13.840397	-0.052389	4.815567
252.763427	8000.072430	13.845402	-0.052424	4.815584
252.668658	8000.045263	13.850407	-0.052406	4.815576
252.471642	8000.038855	13.855411	-0.052369	4.815575
252.564045	8000.030760	13.860416	-0.052387	4.815572
252.679168	8000.013424	13.865421	-0.052408	4.815567
252.781892	8000.035399	13.870426	-0.052428	4.815573
252.731410	8000.004683	13.875431	-0.052418	4.815564
252.832473	8000.037310	13.880435	-0.052437	4.815573
252.911044	8000.066367	13.885440	-0.052452	4.815581
252.650912	8000.031163	13.890445	-0.052404	4.815572
252.724192	8000.045182	13.895450	-0.052417	4.815576
252.744160	8000.020954	13.900455	-0.052421	4.815569
252.695508	8000.036189	13.905459	-0.052412	4.815573
252.527256	8000.037725	13.910464	-0.052381	4.815575
252.402121	8000.026082	13.915469	-0.052358	4.815572
252.582332	8000.035438	13.920474	-0.052391	4.815574
252.542010	7999.991004	13.925479	-0.052384	4.815561
252.604919	8000.018737	13.930483	-0.052396	4.815569
252.632141	8000.018122	13.935488	-0.052401	4.815568
252.639509	8000.016116	13.940493	-0.052402	4.815568
252.622289	8000.032931	13.945498	-0.052399	4.815573
252.727723	7999.999418	13.950503	-0.052419	4.815562
252.666983	8000.032610	13.955507	-0.052408	4.815572
252.773619	8000.022611	13.960512	-0.052428	4.815569
252.807943	8000.013568	13.965517	-0.052434	4.815566
252.869569	8000.048756	13.970522	-0.052446	4.815576
252.718124	8000.023868	13.975527	-0.052418	4.815570
252.808712	8000.040306	13.980531	-0.052435	4.815574
252.802996	8000.018863	13.985536	-0.052434	4.815568
252.725925	8000.010140	13.990541	-0.052420	4.815566
252.622117	8000.057580	13.995546	-0.052400	4.815580
252.552945	8000.029763	14.000551	-0.052388	4.815572
252.710294	8000.044085	14.005555	-0.052417	4.815576
252.589893	8000.019704	14.010560	-0.052395	4.815569
252.540731	8000.008232	14.015565	-0.052386	4.815566
252.569929	8000.034347	14.020570	-0.052391	4.815573
252.591252	8000.012278	14.025575	-0.052395	4.815567
252.626939	8000.048110	14.030579	-0.052402	4.815577
252.483432	8000.030828	14.035584	-0.052375	4.815573
252.439956	8000.011973	14.040589	-0.052367	4.815567
252.427804	8000.033142	14.045594	-0.052365	4.815574
252.680471	8000.014846	14.050599	-0.052412	4.815567
252.624675	8000.027828	14.055603	-0.052402	4.815571
252.457415	8000.008022	14.060608	-0.052371	4.815566
252.571168	8000.015226	14.065613	-0.052392	4.815568
252.791127	8000.023094	14.070618	-0.052433	4.815569
252.833258	7999.999228	14.075623	-0.052441	4.815562
252.571158	8000.024864	14.080627	-0.052393	4.815571
252.576577	8000.033504	14.085632	-0.052394	4.815573
252.627061	8000.033269	14.090637	-0.052403	4.815573
252.556168	8000.040665	14.095642	-0.052390	4.815575
252.634032	8000.039808	14.100647	-0.052405	4.815575
252.559699	8000.019382	14.105651	-0.052391	4.815569
252.530059	8000.037062	14.110656	-0.052386	4.815574
252.602758	8000.029714	14.115661	-0.052399	4.815572
252.632431	8000.062244	14.120666	-0.052405	4.815581
252.629361	8000.010943	14.125671	-0.052404	4.815566
252.660149	8000.039220	14.130675	-0.052410	4.815574
252.768109	8000.032447	14.135680	-0.052430	4.815572
252.578806	8000.022960	14.140685	-0.052395	4.815570
252.672609	8000.049062	14.145690	-0.052413	4.815577
252.785995	8000.018882	14.150695	-0.052434	4.815568
252.949216	8000.047184	14.155699	-0.052465	4.815575
252.715236	8000.055123	14.160704	-0.052421	4.815579
252.667771	8000.038339	14.165709	-0.052412	4.815574
252.754118	8000.038689	14.170714	-0.052429	4.815574
252.615521	8000.010807	14.175719	-0.052403	4.815566
252.716330	8000.018868	14.180723	-0.052422	4.815568
252.887896	8000.035558	14.185728	-0.052454	4.815572
252.597323	7999.999858	14.190733	-0.052400	4.815563
252.610844	8000.051348	14.195738	-0.052402	4.815578
252.675343	8000.021439	14.200743	-0.052414	4.815569
252.749412	8000.011977	14.205747	-0.052428	4.815566
252.791873	8000.021222	14.210752	-0.052436	4.815568
252.552620	8000.008785	14.215757	-0.052392	4.815566
252.678742	8000.030074	14.220762	-0.052415	4.815572
252.601768	8000.030963	14.225767	-0.052401	4.815572
252.556023	8000.016343	14.230771	-0.052393	4.815568
252.555940	8000.009943	14.235776	-0.052393	4.815566
252.529118	8000.000971	14.240781	-0.052388	4.815564
252.500555	8000.025077	14.245786	-0.052383	4.815571
252.592355	7999.994545	14.250791	-0.052400	4.815562
252.762772	8000.025100	14.255795	-0.052432	4.815570
252.955718	7999.075693	14.260800	-0.052467	4.815291

252.635591	7995.956912	14.265805	-0.052406	4.814381
252.562884	7990.516953	14.270810	-0.052389	4.812790
252.540469	7983.881483	14.275815	-0.052380	4.810849
252.355825	7976.620165	14.280819	-0.052341	4.808724
252.661264	7968.987094	14.285824	-0.052393	4.806488
252.595075	7961.190884	14.290829	-0.052376	4.804204
252.649086	7953.378942	14.295834	-0.052381	4.801914
252.606851	7945.370235	14.300839	-0.052368	4.799566
252.692023	7937.457784	14.305843	-0.052379	4.797244
252.693891	7929.401184	14.310848	-0.052374	4.794879
252.366660	7921.410781	14.315853	-0.052308	4.792534
252.387284	7913.384752	14.320858	-0.052307	4.790175
252.353701	7905.426682	14.325863	-0.052295	4.787836
252.280843	7897.342511	14.330867	-0.052277	4.785459
252.173022	7889.442235	14.335872	-0.052252	4.783134
252.114484	7881.346138	14.340877	-0.052236	4.780751
252.150966	7873.437626	14.345882	-0.052237	4.778421
251.971842	7865.392466	14.350887	-0.052199	4.776051
252.060821	7857.365409	14.355891	-0.052210	4.773684
252.084662	7849.400735	14.360896	-0.052210	4.771334
252.072469	7841.364448	14.365901	-0.052202	4.768963
252.025909	7833.408913	14.370906	-0.052188	4.766614
252.106332	7825.363776	14.375911	-0.052198	4.764236
251.967340	7817.431955	14.380915	-0.052167	4.761892
251.865437	7809.330387	14.385920	-0.052143	4.759497
251.838523	7801.413143	14.390925	-0.052133	4.757154
252.019592	7793.377751	14.395930	-0.052162	4.754775
251.948617	7785.331926	14.400935	-0.052143	4.752392
251.940067	7777.287694	14.405939	-0.052137	4.750009
251.961688	7769.351010	14.410944	-0.052136	4.747656
251.801813	7761.307964	14.415949	-0.052101	4.745271
251.890393	7753.379930	14.420954	-0.052112	4.742918
251.756786	7745.331610	14.425959	-0.052082	4.740528
251.706381	7737.359681	14.430963	-0.052068	4.738160
251.653069	7729.357082	14.435968	-0.052053	4.735782
251.795254	7721.331012	14.440973	-0.052074	4.733395
251.508256	7713.290236	14.445978	-0.052015	4.731003
251.388656	7705.297123	14.450983	-0.051988	4.728624
251.375430	7697.309042	14.455987	-0.051980	4.726245
251.624198	7689.332536	14.460992	-0.052022	4.723868
251.526708	7681.309869	14.465997	-0.051998	4.721477
251.521883	7673.331856	14.471002	-0.051992	4.719097
251.443279	7665.324849	14.476007	-0.051973	4.716708
251.370534	7657.283305	14.481011	-0.051954	4.714307
251.353056	7649.297523	14.486016	-0.051946	4.711921
251.272582	7641.286080	14.491021	-0.051925	4.709527
251.317594	7633.313083	14.496026	-0.051929	4.707143
251.288160	7625.292460	14.501031	-0.051918	4.704743
251.157234	7617.286702	14.506035	-0.051889	4.702347
251.263008	7609.319014	14.511040	-0.051903	4.699961
251.055481	7601.319921	14.516045	-0.051859	4.697564
251.001759	7593.299964	14.521050	-0.051844	4.695160
250.896364	7585.320241	14.526055	-0.051820	4.692767
251.020000	7577.286747	14.531059	-0.051837	4.690355
250.907644	7569.304813	14.536064	-0.051811	4.687959
250.951599	7561.252057	14.541069	-0.051815	4.685540
250.918681	7553.328679	14.546074	-0.051803	4.683158
250.919390	7545.296399	14.551079	-0.051798	4.680743
250.798952	7537.295663	14.556083	-0.051771	4.678336
251.022117	7529.321526	14.561088	-0.051807	4.675935
250.824348	7521.236462	14.566093	-0.051765	4.673500
250.821949	7513.126546	14.571098	-0.051760	4.671056
250.846729	7505.215619	14.576103	-0.051759	4.668671
250.758289	7497.212040	14.581107	-0.051738	4.666257
250.693011	7489.267546	14.586112	-0.051720	4.663859
250.574548	7481.203973	14.591117	-0.051693	4.661424
250.841763	7473.249346	14.596122	-0.051738	4.659021
250.633141	7465.248599	14.601127	-0.051694	4.656602
250.649047	7457.238361	14.606131	-0.051692	4.654180
250.947160	7449.250672	14.611136	-0.051742	4.651762
250.688122	7441.223208	14.616141	-0.051689	4.649332
250.772858	7433.255551	14.621146	-0.051699	4.646918
250.768377	7425.186752	14.626151	-0.051693	4.644473
250.435030	7417.259412	14.631155	-0.051626	4.642069
250.492236	7409.215708	14.636160	-0.051632	4.639629
250.315353	7401.218982	14.641165	-0.051594	4.637202
250.452170	7393.199282	14.646170	-0.051614	4.634766
250.442663	7385.204086	14.651175	-0.051607	4.632336
250.513209	7377.151602	14.656179	-0.051615	4.629888
250.536345	7369.216172	14.661184	-0.051615	4.627474
250.295133	7361.178005	14.666189	-0.051564	4.625028
250.341650	7353.231503	14.671194	-0.051568	4.622608
250.307888	7345.160039	14.676199	-0.051557	4.620149
250.147536	7337.215724	14.681203	-0.051522	4.617727
250.087637	7329.209138	14.686208	-0.051505	4.615285
250.089343	7321.168970	14.691213	-0.051501	4.612831
250.194805	7313.133056	14.696218	-0.051515	4.610378
249.953191	7305.164908	14.701223	-0.051465	4.607943
249.947126	7297.136574	14.706227	-0.051459	4.605489
250.119395	7289.205246	14.711232	-0.051486	4.603064
249.977398	7281.181475	14.716237	-0.051454	4.600609
249.799325	7273.225307	14.721242	-0.051416	4.598173
250.046804	7265.205552	14.726247	-0.051457	4.595717
250.070936	7257.112970	14.731251	-0.051456	4.593237
250.141445	7249.101011	14.736256	-0.051464	4.590780
249.782600	7241.108448	14.741261	-0.051392	4.588327
249.950357	7233.103868	14.746266	-0.051418	4.585870
249.749438	7225.110520	14.751271	-0.051376	4.583415
249.644243	7217.111131	14.756275	-0.051351	4.580957
249.834925	7209.166006	14.761280	-0.051382	4.578514
249.730228	7201.158984	14.766285	-0.051357	4.576051
249.584768	7193.129074	14.771290	-0.051325	4.573579
249.590530	7185.105081	14.776295	-0.051321	4.571108
249.637001	7177.142011	14.781299	-0.051324	4.568655
249.559742	7169.140146	14.786304	-0.051305	4.566188
249.495621	7161.149673	14.791309	-0.051288	4.563723
249.541904	7153.142863	14.796314	-0.051291	4.561252
249.516454	7145.151814	14.801319	-0.051281	4.558784
249.385125	7137.141350	14.806323	-0.051252	4.556309
249.596156	7129.123569	14.811328	-0.051286	4.553831
249.540206	7121.058930	14.816333	-0.051270	4.551336
249.458345	7113.106790	14.821338	-0.051250	4.548875
249.389994	7105.082313	14.826343	-0.051232	4.546391
249.292928	7097.110775	14.831347	-0.051209	4.543921
249.283348	7089.151171	14.836352	-0.051202	4.541453
249.133595	7081.120252	14.841357	-0.051169	4.538962
249.249092	7073.166614	14.846362	-0.051186	4.536494
249.199201	7065.129850	14.851367	-0.051171	4.533999
249.143604	7057.091547	14.856371	-0.051156	4.531502
249.191411	7049.091153	14.861376	-0.051160	4.529015
249.068970	7041.116388	14.866381	-0.051132	4.526535
249.112441	7033.089707	14.871386	-0.051135	4.524037
248.977117	7025.157972	14.876391	-0.051104	4.521567
249.033107	7017.094944	14.881395	-0.051110	4.519056
249.101713	7009.177481	14.886400	-0.051117	4.516588
248.892727	7001.056338	14.891405	-0.051073	4.514055
249.063046	6993.015807	14.896410	-0.051100	4.511546
248.980354	6985.046757	14.901415	-0.051079	4.509058
248.878275	6977.040347	14.906419	-0.051055	4.506557
248.795618	6969.046250	14.911424	-0.051035	4.504058
248.825395	6961.054639	14.916429	-0.051035	4.501559
248.734795	6953.069547	14.921434	-0.051013	4.499060
248.724113	6945.118105	14.926439	-0.051006	4.496570
248.605346	6937.036592	14.931443	-0.050979	4.494038
248.779518	6929.070395	14.936448	-0.051006	4.491542
248.447403	6921.045851	14.941453	-0.050939	4.489024
248.313472	6913.052813	14.946458	-0.050909	4.486516
248.425718	6905.054839	14.951463	-0.050925	4.484005
248.416480	6897.057602	14.956467	-0.050918	4.481493
248.252987	6889.067485	14.961472	-0.050883	4.478981
248.356924	6881.078051	14.966477	-0.050897	4.476469
248.470594	6873.032458	14.971482	-0.050913	4.473937
248.420548	6865.047730	14.976487	-0.050898	4.471423
248.532480	6856.997321	14.981491	-0.050914	4.468887
248.441030	6849.052812	14.986496	-0.050892	4.466383
248.213965	6841.014441	14.991501	-0.050845	4.463847
248.349807	6833.056521	14.996506	-0.050865	4.461336
248.277230	6825.049217	15.001511	-0.050846	4.458808
248.095661	6816.991521	15.006515	-0.050807	4.456261
247.997209	6809.034234	15.011520	-0.050784	4.453746
248.054621	6800.991682	15.016525	-0.050789	4.451202
248.080166	6793.019217	15.021530	-0.050789	4.448679
248.158337	6785.011155	15.026535	-0.050798	4.446144
248.133885	6777.026734	15.031539	-0.050789	4.443614
248.365505	6769.062133	15.036544	-0.050827	4.441090
248.044517	6761.054426	15.041549	-0.050762	4.438549
248.041927	6753.021457	15.046554	-0.050756	4.436000
248.093102	6744.971719	15.051559	-0.050761	4.433444
247.903746	6736.945756	15.056563	-0.050720	4.430893
247.910240	6728.997262	15.061568	-0.050717	4.428366
247.820826	6720.935012	15.066573	-0.050695	4.425801
247.688318	6712.999712	15.071578	-0.050665	4.423274
247.764160	6704.998252	15.076583	-0.050674	4.420727
247.661328	6696.982555	15.081587	-0.050650	4.418172
247.826892	6689.005582	15.086592	-0.050675	4.415629
247.637097	6680.978037	15.091597	-0.050635	4.413067
247.482993	6672.940006	15.096602	-0.050601	4.410501
247.670883	6665.006789	15.101607	-0.050631	4.407968
247.510636	6656.957716	15.106611	-0.050596	4.405395
247.369714	6649.045844	15.111616	-0.050565	4.402864
247.339579	6640.948480	15.116621	-0.050554	4.400273
247.522851	6633.047308	15.121626	-0.050583	4.397745
247.457426	6624.995041	15.126631	-0.050566	4.395165
247.263811	6616.980895	15.131635	-0.050525	4.392595
247.317428	6608.937065	15.136640	-0.050529	4.390016
247.193589	6600.987627	15.141645	-0.050501	4.387464
247.388222	6592.939043	15.146650	-0.050532	4.384881
247.440879	6585.042429	15.151655	-0.050537	4.382344
247.266649	6576.938943	15.156659	-0.050500	4.379738
247.299123	6569.045193	15.161664	-0.050501	4.377200
247.187343	6561.003524	15.166669	-0.050475	4.374611
247.192442	6553.004219	15.171674	-0.050470	4.372035
247.250091	6544.961178	15.176679	-0.050476	4.369444
247.160130	6536.973146	15.181683	-0.050454	4.366868
247.185043	6528.986688	15.186688	-0.050454	4.364291
247.022292	6521.024069	15.191693	-0.050418	4.361720
246.988156	6512.962225	15.196698	-0.050407	4.359116
246.993906	6505.016453	15.201703	-0.050403	4.356548
246.913222	6496.930399	15.206707	-0.050383	4.353933
246.859351	6488.863170	15.211712	-0.050367	4.351322
246.704544	6480.883852	15.216717	-0.050333	4.348738
246.773339	6472.912439	15.221722	-0.050341	4.346156
246.630424	6464.933786	15.226727	-0.050309	4.343569
246.468896	6456.966116	15.231731	-0.050274	4.340983
246.680015	6448.990548	15.236736	-0.050309	4.338396
246.619085	6440.963974	15.241741	-0.050292	4.335790
246.426967	6432.941253	15.246746	-0.050251	4.333181
246.592819	6424.927160	15.251751	-0.050277	4.330577
246.492231	6416.943839	15.256755	-0.050253	4.327979
246.541375	6408.950530	15.261760	-0.050257	4.325378
246.369019	6400.947812	15.266765	-0.050220	4.322770
246.555927	6392.965830	15.271770	-0.050250	4.320170
246.231959	6384.993520	15.276775	-0.050184	4.317568
246.166479	6376.919786	15.281779	-0.050167	4.314933
246.283985	6368.930899	15.286784	-0.050184	4.312325
246.278692	6360.869425	15.291789	-0.050178	4.309692
246.236025	6352.924520	15.296794	-0.050164	4.307094
246.481249	6344.920347	15.301799	-0.050205	4.304478
246.525958	6336.914306	15.306803	-0.050208	4.301858
246.545825	6328.962335	15.311808	-0.050207	4.299254
246.111941	6320.956688	15.316813	-0.050121	4.296627
246.327550	6312.910692	15.321818	-0.050156	4.293990
246.243268	6304.916921	15.326823	-0.050135	4.291367
245.978118	6296.868889	15.331827	-0.050081	4.288723
246.229029	6288.924143	15.336832	-0.050122	4.286115
246.395246	6280.925514	15.341837	-0.050148	4.283487
246.103944	6272.916822	15.346842	-0.050089	4.280850
245.920756	6264.962570	15.351847	-0.050050	4.278231
245.990510	6256.889209	15.356851	-0.050057	4.275573
245.965197	6248.896256	15.361856	-0.050048	4.272939
245.982764	6240.845597	15.366861	-0.050046	4.270285
246.147486	6232.869838	15.371866	-0.050071	4.267655
246.050639	6224.880380	15.376871	-0.050048	4.265016
245.850609	6216.902460	15.381875	-0.050006	4.262379
245.908674	6208.890487	15.386880	-0.050012	4.259731
245.883935	6200.935746	15.391885	-0.050002	4.257100
245.729090	6192.899919	15.396890	-0.049968	4.254439
245.862692	6184.878189	15.401895	-0.049988	4.251784
245.957113	6176.875700	15.406899	-0.050000	4.249133
245.917859	6168.891329	15.411904	-0.049988	4.246485
245.634968	6160.912244	15.416909	-0.049930	4.243835
245.510225	6152.921555	15.421914	-0.049902	4.241181
245.599398	6144.921358	15.426919	-0.049913	4.238525
245.345936	6136.939761	15.431923	-0.049861	4.235869
245.508217	6128.965313	15.436928	-0.049886	4.233218
245.495184	6120.884636	15.441933	-0.049878	4.230528
245.528158	6112.915530	15.446938	-0.049879	4.227875
245.490941	6104.910415	15.451943	-0.049867	4.225207
245.440528	6096.903283	15.456947	-0.049853	4.222536
245.623328	6088.919519	15.461952	-0.049882	4.219874
245.434148	6080.963150	15.466957	-0.049841	4.217216
245.440174	6072.931229	15.471962	-0.049837	4.214532
245.273726	6064.947035	15.476967	-0.049801	4.211861
245.097768	6056.880573	15.481971	-0.049763	4.209161
245.030171	6048.940023	15.486976	-0.049746	4.206502
245.087771	6040.918639	15.491981	-0.049751	4.203816
245.218097	6032.941994	15.496986	-0.049771	4.201144
245.184443	6024.974610	15.501991	-0.049759	4.198472
244.983025	6016.959044	15.506995	-0.049717	4.195780
245.080645	6008.850890	15.512000	-0.049730	4.193058
244.869218	6000.821035	15.517005	-0.049685	4.190357
244.916780	5992.867920	15.522010	-0.049689	4.187684
245.088725	5984.887081	15.527015	-0.049716	4.185000
244.890967	5976.933562	15.532019	-0.049674	4.182320
244.892515	5968.863812	15.537024	-0.049669	4.179602
245.081100	5960.919050	15.542029	-0.049699	4.176926
244.719173	5952.908780	15.547034	-0.049627	4.174219
244.802459	5944.913946	15.552039	-0.049637	4.171522
244.625026	5936.864645	15.557043	-0.049599	4.168801
244.873549	5928.898619	15.562048	-0.049640	4.166111
244.765246	5920.896252	15.567053	-0.049615	4.163404
244.601336	5912.913032	15.572058	-0.049579	4.160700
244.692768	5904.941042	15.577063	-0.049591	4.158001
244.680085	5896.880172	15.582067	-0.049583	4.155269
244.516016	5888.874979	15.587072	-0.049548	4.152553
244.429092	5880.857684	15.592077	-0.049526	4.149832
244.398902	5872.865757	15.597082	-0.049516	4.147118
244.574715	5864.880066	15.602087	-0.049543	4.144406
244.516503	5856.907854	15.607091	-0.049527	4.141695
244.539381	5848.866442	15.612096	-0.049527	4.138960
244.429247	5840.908463	15.617101	-0.049501	4.136249
244.276168	5832.892257	15.622106	-0.049467	4.133517
244.460787	5824.875567	15.627111	-0.049497	4.130786
244.174083	5816.863020	15.632115	-0.049438	4.128049
243.969856	5808.886714	15.637120	-0.049395	4.125324
244.200219	5800.876891	15.642125	-0.049433	4.122591
244.215198	5792.869323	15.647130	-0.049430	4.119854
244.126098	5784.942134	15.652135	-0.049409	4.117142
243.943800	5776.883273	15.657139	-0.049370	4.114382
244.111047	5768.852275	15.662144	-0.049396	4.111633
244.076058	5760.854277	15.667149	-0.049384	4.108892
244.034193	5752.860081	15.672154	-0.049371	4.106150
243.775946	5744.913176	15.677159	-0.049318	4.103419
243.736844	5736.900539	15.682163	-0.049306	4.100667
244.008143	5728.953969	15.687168	-0.049351	4.097940
243.862601	5720.872659	15.692173	-0.049319	4.095159
243.689150	5712.875998	15.697178	-0.049281	4.092405
243.632257	5704.871163	15.702183	-0.049266	4.089648
243.631322	5696.919370	15.707187	-0.049260	4.086909
243.700243	5688.926701	15.712192	-0.049268	4.084154
243.564084	5680.956611	15.717197	-0.049238	4.081402
243.421771	5672.940681	15.722202	-0.049206	4.078632
243.776482	5664.942808	15.727207	-0.049267	4.075874
243.615994	5656.895185	15.732211	-0.049232	4.073090
243.592994	5648.892666	15.737216	-0.049223	4.070321
243.556251	5640.916903	15.742221	-0.049211	4.067559
243.523679	5632.902266	15.747226	-0.049199	4.064782
243.510520	5624.969749	15.752231	-0.049192	4.062032
243.300396	5616.926611	15.757235	-0.049148	4.059239
243.385979	5608.986500	15.762240	-0.049159	4.056483
243.348804	5600.924812	15.767245	-0.049146	4.053682
243.320970	5592.896159	15.772250	-0.049136	4.050891
243.295304	5584.914237	15.777255	-0.049126	4.048114
243.192257	5576.899843	15.782259	-0.049102	4.045323
243.235454	5568.943945	15.787264	-0.049105	4.042552
243.073436	5560.921677	15.792269	-0.049070	4.039753
243.016511	5552.971214	15.797274	-0.049054	4.036979
243.085569	5544.917107	15.802279	-0.049062	4.034168
243.115627	5536.785404	15.807283	-0.049062	4.031328
243.019415	5528.876510	15.812288	-0.049039	4.028562
242.791716	5520.892295	15.817293	-0.048992	4.025766
242.780575	5512.899772	15.822298	-0.048984	4.022968
242.981694	5504.891887	15.827303	-0.049017	4.020166
242.756909	5496.935954	15.832307	-0.048970	4.017373
242.838072	5488.933800	15.837312	-0.048980	4.014568
242.699918	5480.897214	15.842317	-0.048949	4.011744
242.596826	5472.880771	15.847322	-0.048925	4.008927
242.740133	5464.930833	15.852327	-0.048946	4.006135
242.602348	5456.923683	15.857331	-0.048915	4.003316
242.597462	5448.933047	15.862336	-0.048909	4.000503
242.574467	5440.936463	15.867341	-0.048900	3.997685
242.626058	5432.880145	15.872346	-0.048905	3.994846
242.620625	5424.873742	15.877351	-0.048898	3.992022
242.624914	5416.866377	15.882355	-0.048894	3.989195
242.740425	5408.901056	15.887360	-0.048911	3.986383
242.375197	5400.913383	15.892365	-0.048837	3.983553
242.440696	5392.880526	15.897370	-0.048844	3.980713
242.473175	5384.925458	15.902375	-0.048845	3.977897
242.447302	5376.920625	15.907379	-0.048835	3.975061
242.613108	5368.904526	15.912384	-0.048861	3.972221
242.483431	5360.886151	15.917389	-0.048832	3.969374
242.491594	5352.954913	15.922394	-0.048828	3.966559
242.483396	5344.959823	15.927399	-0.048822	3.963718
242.219467	5336.959957	15.932403	-0.048768	3.960869
242.203407	5329.018021	15.937408	-0.048759	3.958043
242.105105	5320.972691	15.942413	-0.048736	3.955177
242.091798	5312.902826	15.947418	-0.048728	3.952301
242.095392	5304.922042	15.952423	-0.048724	3.949455
241.961198	5296.929291	15.957427	-0.048694	3.946601
241.963494	5288.974987	15.962432	-0.048689	3.943761
241.953698	5280.965012	15.967437	-0.048682	3.940898
241.898843	5272.991905	15.972442	-0.048667	3.938046
241.831017	5264.989496	15.977447	-0.048649	3.935181
241.911616	5256.931493	15.982451	-0.048659	3.932296
241.951929	5248.953675	15.987456	-0.048661	3.929438
241.716018	5240.972960	15.992461	-0.048612	3.926571
241.693183	5232.983044	15.997466	-0.048603	3.923703
241.879576	5225.028320	16.002471	-0.048633	3.920849
241.738852	5217.030019	16.007475	-0.048601	3.917972
241.851897	5208.990828	16.012480	-0.048617	3.915082
241.991163	5200.952715	16.017485	-0.048638	3.912191
241.743361	5192.956058	16.022490	-0.048587	3.909306
241.508119	5185.023632	16.027495	-0.048538	3.906441
241.610481	5176.960205	16.032499	-0.048552	3.903534
241.582914	5168.975221	16.037504	-0.048542	3.900651
241.310715	5161.017609	16.042509	-0.048486	3.897770
241.414871	5152.980622	16.047514	-0.048500	3.894866
241.505113	5144.974475	16.052519	-0.048512	3.891971
241.357011	5136.936029	16.057523	-0.048479	3.889057
241.494947	5129.015926	16.062528	-0.048500	3.886190
241.470401	5120.998415	16.067533	-0.048490	3.883282
241.457111	5112.953650	16.072538	-0.048482	3.880362
241.229416	5105.065667	16.077543	-0.048435	3.877492
241.049505	5097.005899	16.082547	-0.048396	3.874559
241.251614	5088.730031	16.087552	-0.048429	3.871552
241.133156	5080.844831	16.092557	-0.048402	3.868680
241.107124	5072.885123	16.097562	-0.048392	3.865779
241.129921	5064.979239	16.102567	-0.048391	3.862897
240.962804	5056.946833	16.107571	-0.048355	3.859963
240.927605	5049.001379	16.112576	-0.048343	3.857061
240.905056	5041.004860	16.117581	-0.048334	3.854139
240.788438	5032.953077	16.122586	-0.048307	3.851192
240.756376	5025.017072	16.127591	-0.048296	3.848287
240.717674	5017.002243	16.132595	-0.048283	3.845351
240.817252	5009.030933	16.137600	-0.048297	3.842431
240.613757	5001.032495	16.142605	-0.048254	3.839493
240.566332	4993.062071	16.147610	-0.048240	3.836566
240.712229	4985.038387	16.152615	-0.048262	3.833621
240.508113	4976.977888	16.157619	-0.048219	3.830654
240.578493	4969.025126	16.162624	-0.048227	3.827729
240.590064	4961.010591	16.167629	-0.048224	3.824778
240.585895	4953.047183	16.172634	-0.048218	3.821843
240.549166	4945.074851	16.177639	-0.048206	3.818902
240.502907	4937.040743	16.182643	-0.048192	3.815936
240.478644	4929.062327	16.187648	-0.048183	3.812989
240.587529	4921.021565	16.192653	-0.048198	3.810019
240.345129	4913.023566	16.197658	-0.048148	3.807055
240.338189	4905.095665	16.202663	-0.048141	3.804119
240.178835	4897.120520	16.207667	-0.048107	3.801161
240.162411	4889.117985	16.212672	-0.048098	3.798193
240.113813	4881.116052	16.217677	-0.048084	3.795223
240.255889	4873.053639	16.222682	-0.048106	3.792231
240.275302	4865.036739	16.227687	-0.048104	3.789252
240.218225	4857.017288	16.232691	-0.048088	3.786268
240.364372	4849.056563	16.237696	-0.048110	3.783307
240.248757	4841.062461	16.242701	-0.048084	3.780327
240.204366	4833.093862	16.247706	-0.048070	3.777354
240.228997	4825.068005	16.252711	-0.048070	3.774360
239.999484	4817.078144	16.257715	-0.048022	3.771371
240.114384	4809.070413	16.262720	-0.048038	3.768381
239.970340	4801.107337	16.267725	-0.048006	3.765399
239.939849	4793.112001	16.272730	-0.047996	3.762405
240.001561	4785.128210	16.277735	-0.048002	3.759416
239.749048	4777.130171	16.282739	-0.047950	3.756411
239.769074	4769.095178	16.287744	-0.047948	3.753397
239.777350	4761.079001	16.292749	-0.047945	3.750386
239.620396	4753.077055	16.297754	-0.047911	3.747375
239.698283	4745.082717	16.302759	-0.047920	3.744370
239.522915	4737.139644	16.307763	-0.047882	3.741376
239.745142	4729.104316	16.312768	-0.047918	3.738353
239.764715	4721.101406	16.317773	-0.047917	3.735336
239.661430	4713.125129	16.322778	-0.047893	3.732324
239.679578	4705.103025	16.327783	-0.047891	3.729295
239.480247	4697.149979	16.332787	-0.047849	3.726284
239.584535	4689.157688	16.337792	-0.047863	3.723263
239.643740	4681.156595	16.342797	-0.047869	3.720235
239.585360	4673.195073	16.347802	-0.047853	3.717217
239.561753	4665.171151	16.352807	-0.047843	3.714174
239.391553	4657.046524	16.357811	-0.047807	3.711086
239.467235	4649.091102	16.362816	-0.047816	3.708066
239.374590	4641.121051	16.367821	-0.047793	3.705034
239.151883	4633.170143	16.372826	-0.047747	3.702004
239.222533	4625.200128	16.377831	-0.047755	3.698971
239.335926	4617.181414	16.382835	-0.047771	3.695918
239.230953	4609.193452	16.387840	-0.047746	3.692868
239.054787	4601.156334	16.392845	-0.047708	3.689796
238.907238	4593.191901	16.397850	-0.047676	3.686750
238.930947	4585.235011	16.402855	-0.047675	3.683708
238.967090	4577.213729	16.407859	-0.047677	3.680639
238.858152	4569.273171	16.412864	-0.047651	3.677595
239.163065	4561.199213	16.417869	-0.047703	3.674508
239.102643	4553.192206	16.422874	-0.047686	3.671435
239.126073	4545.232624	16.427879	-0.047686	3.668379
238.847763	4537.187143	16.432883	-0.047629	3.665280
239.037157	4529.243534	16.437888	-0.047659	3.662230
238.917300	4521.248804	16.442893	-0.047632	3.659150
238.785388	4513.247916	16.447898	-0.047602	3.656064
238.996119	4505.240990	16.452903	-0.047636	3.652982
238.839971	4497.188203	16.457907	-0.047602	3.649871
238.806516	4489.246250	16.462912	-0.047590	3.646802
238.804502	4481.250712	16.467917	-0.047585	3.643712
238.685538	4473.255516	16.472922	-0.047558	3.640615
238.656313	4465.317386	16.477927	-0.047547	3.637541
238.593261	4457.261105	16.482931	-0.047530	3.634417
238.515493	4449.224877	16.487936	-0.047511	3.631297
238.576301	4441.214863	16.492941	-0.047517	3.628190
238.317393	4433.225228	16.497946	-0.047464	3.625078
238.381869	4425.282476	16.502951	-0.047471	3.621991
238.506948	4417.270849	16.507955	-0.047489	3.618876
238.411616	4409.297642	16.512960	-0.047466	3.615768
238.233432	4401.305986	16.517965	-0.047428	3.612647
238.325675	4393.266950	16.522970	-0.047440	3.609512
238.279475	4385.313424	16.527975	-0.047426	3.606405
238.141266	4377.315065	16.532979	-0.047395	3.603274
238.287369	4369.352046	16.537984	-0.047417	3.600163
238.202247	4361.388524	16.542989	-0.047396	3.597042
237.985469	4353.353041	16.547994	-0.047351	3.593887
238.015656	4345.349076	16.552999	-0.047351	3.590748
237.983017	4337.368566	16.558003	-0.047340	3.587614
238.121861	4329.346090	16.563008	-0.047361	3.584465
237.821140	4321.416506	16.568013	-0.047300	3.581338
237.870517	4313.393960	16.573018	-0.047304	3.578181
237.994169	4305.385722	16.578023	-0.047322	3.575030
237.769627	4297.360148	16.583027	-0.047275	3.571858
237.687750	4289.382722	16.588032	-0.047254	3.568707
237.795379	4281.371570	16.593037	-0.047269	3.565546
237.681926	4273.418531	16.598042	-0.047243	3.562398
237.620102	4265.423021	16.603047	-0.047227	3.559232
237.619883	4257.438752	16.608051	-0.047221	3.556069
237.631028	4249.351336	16.613056	-0.047218	3.552863
237.570037	4241.334797	16.618061	-0.047202	3.549680
237.477907	4233.330167	16.623066	-0.047180	3.546498
237.649031	4225.374255	16.628071	-0.047206	3.543341
237.442868	4217.397261	16.633075	-0.047163	3.540161
237.615711	4209.436576	16.638080	-0.047190	3.536996
237.686819	4201.417823	16.643085	-0.047198	3.533801
237.575913	4193.380975	16.648090	-0.047172	3.530592
237.532874	4185.452615	16.653095	-0.047159	3.527424
237.382303	4177.408422	16.658099	-0.047126	3.524205
237.479524	4169.481444	16.663104	-0.047139	3.521036
237.249064	4161.500135	16.668109	-0.047091	3.517834
237.231419	4153.464714	16.673114	-0.047083	3.514613
237.260961	4145.503055	16.678119	-0.047083	3.511420
237.119402	4137.466229	16.683123	-0.047052	3.508188
237.087139	4129.468027	16.688128	-0.047040	3.504973
237.152416	4121.528584	16.693133	-0.047048	3.501782
236.886643	4113.553871	16.698138	-0.046993	3.498562
237.027305	4105.551094	16.703143	-0.047014	3.495342
237.017631	4097.528692	16.708147	-0.047007	3.492105
236.993857	4089.530298	16.713152	-0.046998	3.488875
236.852343	4081.533122	16.718157	-0.046966	3.485639
236.725617	4073.570054	16.723162	-0.046937	3.482414
237.078625	4065.579676	16.728167	-0.046998	3.479190
236.949960	4057.601513	16.733171	-0.046969	3.475953
236.907679	4049.576303	16.738176	-0.046956	3.472697
237.027306	4041.550395	16.743181	-0.046973	3.469442
236.885186	4033.554348	16.748186	-0.046942	3.466188
236.613820	4025.628363	16.753191	-0.046886	3.462955
236.653384	4017.580028	16.758195	-0.046888	3.459679
236.809323	4009.621086	16.763200	-0.046912	3.456441
236.545642	4001.625247	16.768205	-0.046858	3.453171
236.451616	3993.585988	16.773210	-0.046835	3.449885
236.620815	3985.648461	16.778215	-0.046862	3.446647
236.450103	3977.617697	16.783219	-0.046825	3.443356
236.393262	3969.657848	16.788224	-0.046809	3.440094
236.312108	3961.661114	16.793229	-0.046789	3.436814
236.557477	3953.645424	16.798234	-0.046830	3.433534
236.405444	3945.644699	16.803239	-0.046796	3.430243
236.315688	3937.658011	16.808243	-0.046774	3.426957
236.512416	3929.647153	16.813248	-0.046806	3.423668
236.324299	3921.693780	16.818253	-0.046766	3.420386
236.218500	3913.724685	16.823258	-0.046741	3.417097
236.421320	3905.717367	16.828263	-0.046774	3.413800
236.003913	3897.712460	16.833267	-0.046691	3.410480
236.007453	3889.731887	16.838272	-0.046686	3.407180
236.109827	3881.740257	16.843277	-0.046700	3.403877
236.101684	3873.729412	16.848282	-0.046694	3.400558
235.972488	3865.813289	16.853287	-0.046664	3.397271
235.800452	3857.764133	16.858291	-0.046627	3.393924
236.029068	3849.647255	16.863296	-0.046665	3.390560
235.941195	3841.698563	16.868301	-0.046643	3.387251
235.594236	3833.745833	16.873306	-0.046574	3.383929
235.703462	3825.794664	16.878311	-0.046589	3.380619
235.620705	3817.814406	16.883315	-0.046568	3.377288
235.596746	3809.793716	16.888320	-0.046559	3.373938
235.423058	3801.819902	16.893325	-0.046521	3.370600
235.625947	3793.792814	16.898330	-0.046554	3.367249
235.515818	3785.825761	16.903335	-0.046528	3.363909
235.448553	3777.842901	16.908339	-0.046511	3.360560
235.316879	3769.893652	16.913344	-0.046481	3.357220
235.573479	3761.857990	16.918349	-0.046524	3.353854
235.417088	3753.814749	16.923354	-0.046490	3.350466
235.364564	3745.856731	16.928359	-0.046475	3.347115
235.275258	3737.861020	16.933363	-0.046453	3.343744
235.251038	3729.907715	16.938368	-0.046443	3.340389
235.218633	3721.920257	16.943373	-0.046432	3.337016
235.169728	3713.893599	16.948378	-0.046418	3.333622
235.139780	3705.885284	16.953383	-0.046407	3.330233
235.028552	3697.895219	16.958387	-0.046381	3.326846
235.010483	3689.936076	16.963392	-0.046373	3.323472
235.167650	3681.955611	16.968397	-0.046397	3.320092
234.964436	3673.989320	16.973402	-0.046354	3.316700
234.879666	3665.970151	16.978407	-0.046333	3.313288
234.884501	3657.919081	16.983411	-0.046329	3.309861
234.931519	3649.949502	16.988416	-0.046333	3.306468
234.720852	3641.994218	16.993421	-0.046288	3.303067
235.026498	3633.965314	16.998426	-0.046340	3.299651
234.949052	3626.054068	17.003431	-0.046321	3.296267
234.859464	3618.019328	17.008435	-0.046299	3.292826
234.807197	3610.032667	17.013440	-0.046284	3.289404
234.663166	3602.073529	17.018445	-0.046252	3.285986
234.740427	3594.056237	17.023450	-0.046261	3.282549
234.876416	3586.093568	17.028455	-0.046282	3.279133
234.818664	3578.124769	17.033459	-0.046266	3.275704
234.723516	3570.098885	17.038464	-0.046243	3.272245
234.594400	3562.070149	17.043469	-0.046214	3.268780
234.636018	3554.071304	17.048474	-0.046216	3.265331
234.626896	3546.138276	17.053479	-0.046210	3.261904
234.383498	3538.155661	17.058483	-0.046159	3.258444
234.397511	3530.147202	17.063488	-0.046157	3.254978
234.669028	3522.123580	17.068493	-0.046202	3.251513
234.521904	3514.127552	17.073498	-0.046170	3.248039
234.368584	3506.150069	17.078503	-0.046136	3.244569
234.319022	3498.213948	17.083507	-0.046122	3.241118
234.375472	3490.214082	17.088512	-0.046127	3.237639
234.127165	3482.219602	17.093517	-0.046076	3.234147
234.093632	3474.157342	17.098522	-0.046064	3.230630
234.239404	3466.154335	17.103527	-0.046086	3.227142
234.132770	3458.184236	17.108531	-0.046062	3.223655
234.081452	3450.233323	17.113536	-0.046047	3.220175
234.258145	3442.243256	17.118541	-0.046075	3.216683
233.966985	3434.253863	17.123546	-0.046015	3.213168
234.064113	3426.248821	17.128551	-0.046028	3.209659
233.979665	3418.287405	17.133555	-0.046008	3.206157
233.934748	3410.304031	17.138560	-0.045994	3.202643
233.906132	3402.334274	17.143565	-0.045984	3.199133
233.864078	3394.341293	17.148570	-0.045971	3.195607
234.030632	3386.313948	17.153575	-0.045997	3.192072
233.725487	3378.330566	17.158579	-0.045935	3.188532
233.667827	3370.335349	17.163584	-0.045919	3.184993
233.622438	3362.382401	17.168589	-0.045905	3.181469
233.607440	3354.398769	17.173594	-0.045897	3.177930
233.527468	3346.430998	17.178599	-0.045877	3.174390
233.619066	3338.381868	17.183603	-0.045889	3.170818
233.516987	3330.420111	17.188608	-0.045865	3.167272
233.502081	3322.432955	17.193613	-0.045857	3.163715
233.260055	3314.477526	17.198618	-0.045807	3.160158
233.525969	3306.475508	17.203623	-0.045852	3.156599
233.328389	3298.456302	17.208627	-0.045810	3.153007
233.456701	3290.434059	17.213632	-0.045828	3.149424
233.490940	3282.455167	17.218637	-0.045830	3.145853
233.375821	3274.491604	17.223642	-0.045803	3.142277
233.225652	3266.549643	17.228647	-0.045770	3.138706
233.094823	3258.546153	17.233651	-0.045741	3.135104
233.158032	3250.531417	17.238656	-0.045747	3.131501
233.192375	3242.545354	17.243661	-0.045749	3.127906
233.024278	3234.531054	17.248666	-0.045712	3.124285
233.104665	3226.630748	17.253671	-0.045722	3.120722
233.047133	3218.636451	17.258675	-0.045706	3.117106
232.845516	3210.655458	17.263680	-0.045664	3.113486
232.971161	3202.609201	17.268685	-0.045682	3.109847
232.925864	3194.622404	17.273690	-0.045668	3.106222
232.929714	3186.680577	17.278695	-0.045664	3.102616
232.640489	3178.692269	17.283699	-0.045605	3.098972
232.702445	3170.683700	17.288704	-0.045612	3.095330
232.608669	3162.700208	17.293709	-0.045589	3.091687
232.600784	3154.683313	17.298714	-0.045582	3.088030
232.696177	3146.702372	17.303719	-0.045595	3.084389
232.765548	3138.768242	17.308723	-0.045603	3.080764
232.446839	3130.805780	17.313728	-0.045538	3.077104
232.702414	3122.748293	17.318733	-0.045581	3.073422
232.745143	3114.686657	17.323738	-0.045584	3.069724
232.517676	3106.763463	17.328743	-0.045536	3.066073
232.494234	3098.767246	17.333747	-0.045527	3.062394
232.425792	3090.821167	17.338752	-0.045509	3.058731
232.212161	3082.874507	17.343757	-0.045464	3.055056
232.409175	3074.834480	17.348762	-0.045496	3.051353
232.444697	3066.855845	17.353767	-0.045497	3.047667
232.297851	3058.869937	17.358771	-0.045465	3.043964
232.127353	3050.927915	17.363776	-0.045428	3.040275
232.130546	3042.964179	17.368781	-0.045423	3.036581
232.178410	3034.924897	17.373786	-0.045427	3.032849
232.141447	3026.929799	17.378791	-0.045415	3.029129
232.035346	3018.957105	17.383795	-0.045390	3.025411
232.100621	3010.988430	17.388800	-0.045397	3.021699
232.421749	3002.982047	17.393805	-0.045452	3.017977
232.156306	2994.995409	17.398810	-0.045398	3.014231
232.154754	2987.017818	17.403815	-0.045392	3.010498
231.973807	2979.044344	17.408819	-0.045353	3.006753
231.947548	2971.059953	17.413824	-0.045343	3.003006
231.985253	2963.101377	17.418829	-0.045345	2.999270
231.808048	2955.128978	17.423834	-0.045307	2.995512
231.881882	2947.110279	17.428839	-0.045316	2.991739
231.909993	2939.093272	17.433843	-0.045316	2.987961
231.905036	2931.107752	17.438848	-0.045310	2.984191
231.651989	2923.195045	17.443853	-0.045258	2.980438
231.726344	2915.184341	17.448858	-0.045267	2.976650
231.671961	2907.203478	17.453863	-0.045251	2.972865
231.698374	2899.192596	17.458867	-0.045251	2.969065
231.464684	2891.243493	17.463872	-0.045203	2.965277
231.549236	2883.268513	17.468877	-0.045213	2.961487
231.513733	2875.275353	17.473882	-0.045201	2.957678
231.353680	2867.335377	17.478887	-0.045167	2.953883
231.167463	2859.303331	17.483891	-0.045127	2.950038
231.449414	2851.292529	17.488896	-0.045174	2.946222
231.462597	2843.319138	17.493901	-0.045172	2.942405
231.101643	2835.390209	17.498906	-0.045099	2.938585
231.110337	2827.404271	17.503911	-0.045096	2.934751
231.268003	2819.356058	17.508915	-0.045120	2.930891
231.057895	2811.405837	17.513920	-0.045076	2.927054
231.249513	2803.425456	17.518925	-0.045106	2.923218
230.984183	2795.458963	17.523930	-0.045052	2.919359
230.879840	2787.522923	17.528935	-0.045027	2.915519
230.862915	2779.424006	17.533939	-0.045019	2.911599
230.826405	2771.434107	17.538944	-0.045007	2.907726
230.865695	2763.479305	17.543949	-0.045009	2.903869
230.726604	2755.500823	17.548954	-0.044978	2.899985
230.613737	2747.575093	17.553959	-0.044952	2.896124
230.775775	2739.535353	17.558963	-0.044977	2.892216
230.477415	2731.589524	17.563968	-0.044917	2.888324
230.675055	2723.587864	17.568973	-0.044948	2.884427
230.542609	2715.649662	17.573978	-0.044919	2.880537
230.536602	2707.687110	17.578983	-0.044912	2.876637
230.495876	2699.674356	17.583987	-0.044900	2.872705
230.486102	2691.665312	17.588992	-0.044893	2.868771
230.449023	2683.703315	17.593997	-0.044881	2.864854
230.254502	2675.753460	17.599002	-0.044840	2.860928
230.278871	2667.802618	17.604007	-0.044839	2.857009
230.304148	2659.786754	17.609011	-0.044839	2.853052
230.192917	2651.782915	17.614016	-0.044813	2.849088
230.134253	2643.812676	17.619021	-0.044797	2.845138
230.120450	2635.839639	17.624026	-0.044789	2.841184
229.998320	2627.895671	17.629031	-0.044761	2.837232
229.962613	2619.885869	17.634035	-0.044749	2.833247
230.029587	2611.873143	17.639040	-0.044757	2.829261
230.053341	2603.888494	17.644045	-0.044756	2.825281
229.920030	2595.935548	17.649050	-0.044726	2.821302
229.995421	2587.958128	17.654055	-0.044735	2.817317
230.159591	2579.945632	17.659059	-0.044761	2.813314
229.910306	2571.968339	17.664064	-0.044709	2.809299
229.900985	2564.009741	17.669069	-0.044702	2.805302
229.865420	2556.056834	17.674074	-0.044691	2.801300
229.859439	2548.109414	17.679079	-0.044684	2.797297
229.622884	2540.117791	17.684083	-0.044635	2.793252
229.468199	2532.133941	17.689088	-0.044601	2.789211
229.631940	2524.138959	17.694093	-0.044627	2.785176
229.431246	2516.186155	17.699098	-0.044584	2.781136
229.479940	2508.216579	17.704103	-0.044588	2.777095
229.632076	2500.206589	17.709107	-0.044611	2.773035
229.526930	2492.215630	17.714112	-0.044587	2.768963
229.391003	2484.268863	17.719117	-0.044556	2.764905
229.305642	2476.306508	17.724122	-0.044535	2.760837
229.459408	2468.332120	17.729127	-0.044559	2.756771
229.314765	2460.300898	17.734131	-0.044527	2.752652
229.193221	2452.294270	17.739136	-0.044499	2.748541
229.242277	2444.333637	17.744141	-0.044503	2.744457
229.053194	2436.394169	17.749146	-0.044463	2.740364
229.118296	2428.422628	17.754151	-0.044470	2.736263
229.250760	2420.404190	17.759155	-0.044489	2.732137
229.189007	2412.448047	17.764160	-0.044473	2.728024
229.098524	2404.489260	17.769165	-0.044451	2.723902
228.862750	2396.544229	17.774170	-0.044402	2.719772
229.238971	2388.568397	17.779175	-0.044467	2.715657
229.145352	2380.562756	17.784179	-0.044444	2.711492
229.004095	2372.581768	17.789184	-0.044413	2.707330
229.001542	2364.628213	17.794189	-0.044407	2.703185
228.965834	2356.656179	17.799194	-0.044396	2.699021
228.793091	2348.718924	17.804199	-0.044358	2.694861
228.716728	2340.715675	17.809203	-0.044339	2.690665
228.820671	2332.724595	17.814208	-0.044353	2.686481
228.723908	2324.786209	17.819213	-0.044330	2.682306
228.448700	2316.835005	17.824218	-0.044274	2.678105
228.504411	2308.836745	17.829223	-0.044279	2.673895
228.530817	2300.820325	17.834227	-0.044279	2.669666
228.591813	2292.846609	17.839232	-0.044285	2.665455
228.494387	2284.902998	17.844237	-0.044262	2.661244
228.489819	2276.911259	17.849242	-0.044256	2.657006
228.270796	2268.963192	17.854247	-0.044210	2.652771
228.512022	2260.948702	17.859251	-0.044250	2.648523
228.365455	2252.995373	17.864256	-0.044218	2.644276
228.449236	2245.046185	17.869261	-0.044228	2.640040
228.217238	2237.107709	17.874266	-0.044180	2.635781
228.225374	2229.116474	17.879271	-0.044176	2.631503
228.237623	2221.103104	17.884275	-0.044174	2.627207
228.072678	2213.161035	17.889280	-0.044138	2.622930
227.972755	2205.212076	17.894285	-0.044114	2.618647
227.900647	2197.220630	17.899290	-0.044096	2.614336
227.822853	2189.244267	17.904295	-0.044076	2.610025
227.743255	2181.281924	17.909299	-0.044056	2.605715
227.832970	2173.306520	17.914304	-0.044068	2.601401
227.767693	2165.376853	17.919309	-0.044050	2.597095
227.739064	2157.283570	17.924314	-0.044040	2.592696
227.939818	2149.207704	17.929319	-0.044072	2.588314
227.832498	2141.276696	17.934323	-0.044047	2.583982
227.787114	2133.366975	17.939328	-0.044034	2.579659
227.710539	2125.439105	17.944333	-0.044014	2.575317
227.613040	2117.463811	17.949338	-0.043991	2.570940
227.736907	2109.476504	17.954343	-0.044009	2.566564
227.442651	2101.570876	17.959347	-0.043949	2.562197
227.318600	2093.629332	17.964352	-0.043921	2.557814
227.381819	2085.656539	17.969357	-0.043928	2.553419
227.290726	2077.662548	17.974362	-0.043906	2.548995
227.409691	2069.676072	17.979367	-0.043923	2.544581
227.459445	2061.725682	17.984371	-0.043927	2.540175
227.286295	2053.762726	17.989376	-0.043889	2.535739
227.303567	2045.795938	17.994381	-0.043888	2.531306
227.398210	2037.804943	17.999386	-0.043900	2.526858
227.333183	2029.878562	18.004391	-0.043883	2.522426
227.231900	2021.921735	18.009395	-0.043859	2.517967
227.309037	2013.924699	18.014400	-0.043868	2.513490
227.035569	2005.977791	18.019405	-0.043812	2.509008
226.986396	1997.983079	18.024410	-0.043798	2.504507
226.953147	1990.041944	18.029415	-0.043787	2.500030
226.777113	1982.102005	18.034419	-0.043749	2.495535
226.678568	1974.111295	18.039424	-0.043725	2.491008
226.793317	1966.131743	18.044429	-0.043742	2.486496
226.917343	1958.173913	18.049434	-0.043760	2.481988
226.947846	1950.214364	18.054439	-0.043760	2.477464
226.885588	1942.267989	18.059443	-0.043744	2.472932
226.919390	1934.271771	18.064448	-0.043745	2.468371
226.716131	1926.340892	18.069453	-0.043702	2.463821
226.471999	1918.403176	18.074458	-0.043651	2.459256
226.641429	1910.422388	18.079463	-0.043678	2.454688
226.529583	1902.451728	18.084467	-0.043652	2.450096
226.298779	1894.508718	18.089472	-0.043604	2.445503
226.424195	1886.542834	18.094477	-0.043622	2.440915
226.582585	1878.557562	18.099482	-0.043647	2.436310
226.591886	1870.547994	18.104487	-0.043643	2.431670
226.230274	1862.597323	18.109491	-0.043571	2.427027
226.240752	1854.633242	18.114496	-0.043568	2.422396
226.091863	1846.729576	18.119501	-0.043535	2.417780
225.895295	1838.765679	18.124506	-0.043493	2.413115
226.125892	1830.764006	18.129511	-0.043531	2.408453
225.978390	1822.823458	18.134515	-0.043498	2.403787
226.056585	1814.868602	18.139520	-0.043508	2.399122
225.993244	1806.939564	18.144525	-0.043491	2.394452
226.019162	1798.935267	18.149530	-0.043491	2.389736
226.000673	1790.983842	18.154535	-0.043482	2.385037
225.844686	1783.042273	18.159539	-0.043448	2.380325
225.698615	1775.112300	18.164544	-0.043416	2.375611
225.634310	1767.144384	18.169549	-0.043399	2.370871
225.587317	1759.170460	18.174554	-0.043385	2.366120
225.572609	1751.223905	18.179559	-0.043377	2.361378
225.639201	1743.282860	18.184563	-0.043384	2.356636
225.700714	1735.281370	18.189568	-0.043391	2.351848
225.429041	1727.367984	18.194573	-0.043335	2.347076
225.414848	1719.386695	18.199578	-0.043327	2.342275
225.406330	1711.453342	18.204583	-0.043321	2.337493
225.179974	1703.504378	18.209587	-0.043274	2.332674
225.073042	1695.529696	18.214592	-0.043249	2.327839
225.227995	1687.575539	18.219597	-0.043272	2.323028
225.166494	1679.622390	18.224602	-0.043256	2.318190
225.099238	1671.689220	18.229607	-0.043238	2.313353
225.088932	1663.705084	18.234611	-0.043231	2.308480
225.038548	1655.741767	18.239616	-0.043217	2.303606
225.176546	1647.811701	18.244621	-0.043237	2.298758
225.055350	1639.855181	18.249626	-0.043210	2.293861
225.159871	1631.886165	18.254631	-0.043224	2.288966
224.984129	1623.960111	18.259635	-0.043186	2.284062
225.044226	1616.011309	18.264640	-0.043192	2.279154
225.062866	1608.072972	18.269645	-0.043191	2.274239
224.758837	1600.062812	18.274650	-0.043129	2.269240
224.435884	1592.152320	18.279655	-0.043064	2.264291
224.612448	1584.183983	18.284659	-0.043092	2.259338
224.479264	1576.247100	18.289664	-0.043062	2.254367
224.364113	1568.300393	18.294669	-0.043035	2.249380
224.341962	1560.339530	18.299674	-0.043026	2.244381
224.498403	1552.401961	18.304679	-0.043050	2.239402
224.339600	1544.471580	18.309683	-0.043015	2.234388
224.236431	1536.507137	18.314688	-0.042991	2.229346
224.376673	1528.541914	18.319693	-0.043012	2.224314
224.359162	1520.602989	18.324698	-0.043004	2.219273
224.177863	1512.685267	18.329703	-0.042965	2.214220
224.397969	1504.686935	18.334707	-0.043001	2.209139
224.121214	1496.788567	18.339712	-0.042944	2.204067
224.212277	1488.854462	18.344717	-0.042956	2.198992
224.033662	1480.911138	18.349722	-0.042918	2.193876
224.229967	1472.916440	18.354727	-0.042949	2.188748
223.972000	1464.994541	18.359731	-0.042896	2.183614
224.000146	1457.049877	18.364736	-0.042896	2.178480
223.990512	1449.113398	18.369741	-0.042890	2.173335
223.839968	1441.173754	18.374746	-0.042856	2.168163
223.803192	1433.237177	18.379751	-0.042845	2.162990
223.591970	1425.335881	18.384755	-0.042800	2.157813
223.744856	1417.343536	18.389760	-0.042824	2.152597
223.715426	1409.411485	18.394765	-0.042813	2.147391
223.421960	1401.489784	18.399770	-0.042753	2.142154
223.606456	1393.545585	18.404775	-0.042783	2.136935
223.532850	1385.607926	18.409779	-0.042764	2.131683
223.358939	1377.667576	18.414784	-0.042726	2.126407
223.470821	1369.728659	18.419789	-0.042742	2.121145
223.327740	1361.805120	18.424794	-0.042710	2.115857
223.325426	1353.805468	18.429799	-0.042705	2.110517
223.238907	1345.866874	18.434803	-0.042684	2.105197
223.235573	1337.926820	18.439808	-0.042678	2.099871
223.265586	1330.017591	18.444813	-0.042678	2.094555
223.065818	1322.077352	18.449818	-0.042636	2.089182
223.091549	1314.163871	18.454823	-0.042636	2.083835
223.150775	1306.231736	18.459827	-0.042642	2.078466
223.122477	1298.290800	18.464832	-0.042632	2.073067
223.087888	1290.358192	18.469837	-0.042620	2.067660
223.214505	1282.401100	18.474842	-0.042639	2.062238
222.804634	1274.533291	18.479847	-0.042557	2.056809
222.963420	1266.577130	18.484851	-0.042582	2.051362
222.988466	1258.627380	18.489856	-0.042581	2.045891
222.766629	1250.749792	18.494861	-0.042535	2.040431
222.648503	1242.829538	18.499866	-0.042508	2.034937
222.697036	1234.868463	18.504871	-0.042512	2.029417
222.592874	1226.933135	18.509875	-0.042487	2.023883
222.468639	1219.029229	18.514880	-0.042459	2.018355
222.582797	1211.083737	18.519885	-0.042475	2.012807
222.551857	1203.141751	18.524890	-0.042465	2.007231
222.491084	1195.242646	18.529895	-0.042448	2.001666
222.076148	1187.377442	18.534899	-0.042366	1.996073
222.146303	1179.406547	18.539904	-0.042374	1.990440
222.255865	1171.464349	18.544909	-0.042389	1.984816
222.116181	1163.565472	18.549914	-0.042358	1.979180
222.008793	1155.661208	18.554919	-0.042333	1.973528
222.073497	1147.713434	18.559923	-0.042340	1.967846
221.921181	1139.808392	18.564928	-0.042307	1.962156
221.939689	1131.907942	18.569933	-0.042305	1.956470
221.790617	1123.951909	18.574938	-0.042272	1.950710
221.906603	1115.993235	18.579943	-0.042289	1.944960
221.873547	1108.101623	18.584947	-0.042278	1.939225
221.880098	1100.166620	18.589952	-0.042274	1.933446
221.754109	1092.277414	18.594957	-0.042245	1.927668
221.567561	1084.377469	18.599962	-0.042205	1.921858
221.615929	1076.471131	18.604967	-0.042209	1.916052
221.700899	1068.526490	18.609971	-0.042220	1.910204
221.388611	1060.638005	18.614976	-0.042157	1.904336
221.466244	1052.731108	18.619981	-0.042166	1.898479
221.460168	1044.803623	18.624986	-0.042160	1.892579
221.331910	1036.903744	18.629991	-0.042131	1.886668
221.219196	1029.016757	18.634995	-0.042105	1.880749
221.118292	1021.116134	18.640000	-0.042081	1.874803
221.197209	1013.186915	18.645005	-0.042091	1.868837
221.181758	1005.265582	18.650010	-0.042083	1.862847
221.065079	997.388479	18.655015	-0.042056	1.856860
221.032740	989.471696	18.660019	-0.042045	1.850832
220.740470	981.582587	18.665024	-0.041986	1.844776
220.841786	973.690902	18.670029	-0.042000	1.838744
220.689683	965.792357	18.675034	-0.041966	1.832657
220.652224	957.890371	18.680039	-0.041954	1.826560
220.521036	950.000599	18.685043	-0.041925	1.820442
220.704872	942.076560	18.690048	-0.041954	1.814313
220.617799	934.180129	18.695053	-0.041933	1.808153
220.502228	926.289725	18.700058	-0.041906	1.801973
220.632217	918.398347	18.705063	-0.041925	1.795801
220.615679	910.450709	18.710067	-0.041917	1.789546
220.397764	902.571575	18.715072	-0.041871	1.783298
220.392108	894.703726	18.720077	-0.041865	1.777063
220.340767	886.800602	18.725082	-0.041851	1.770772
220.301247	878.918252	18.730087	-0.041838	1.764477
220.178612	871.062593	18.735091	-0.041811	1.758171
220.227096	863.156689	18.740096	-0.041815	1.751822
220.119176	855.281021	18.745101	-0.041789	1.745456
220.080262	847.405242	18.750106	-0.041777	1.739074
220.111254	839.519400	18.755111	-0.041778	1.732670
220.032839	831.645615	18.760115	-0.041758	1.726238
219.934275	823.772774	18.765120	-0.041735	1.719780
220.107779	815.881608	18.770125	-0.041762	1.713318
219.924702	807.996472	18.775130	-0.041723	1.706790
219.946515	800.120968	18.780135	-0.041722	1.700271
219.827076	792.272783	18.785139	-0.041695	1.693732
219.666013	784.396767	18.790144	-0.041660	1.687138
219.806074	776.509540	18.795149	-0.041681	1.680549
219.429676	768.700465	18.800154	-0.041606	1.673932
219.317700	760.826748	18.805159	-0.041580	1.667268
219.586578	752.913564	18.810163	-0.041625	1.660596
219.498679	745.066100	18.815168	-0.041603	1.653904
219.363609	737.218928	18.820173	-0.041573	1.647179
219.212623	729.364300	18.825178	-0.041540	1.640418
219.344918	721.480284	18.830183	-0.041560	1.633643
219.134733	713.600530	18.835187	-0.041516	1.626795
218.998888	705.757802	18.840192	-0.041485	1.619961
219.180794	697.883761	18.845197	-0.041514	1.613115
219.249751	689.996837	18.850202	-0.041522	1.606213
219.122382	682.187590	18.855207	-0.041493	1.599322
218.976487	674.364296	18.860211	-0.041461	1.592386
218.835309	666.507044	18.865216	-0.041430	1.585390
218.661439	658.715846	18.870221	-0.041392	1.578417
218.532679	650.854884	18.875226	-0.041363	1.571357
218.604356	642.999352	18.880231	-0.041372	1.564299
218.587004	635.175765	18.885235	-0.041364	1.557225
218.414622	627.334042	18.890240	-0.041326	1.550080
218.628087	619.466542	18.895245	-0.041361	1.542935
218.430234	611.656211	18.900250	-0.041319	1.535748
218.276526	603.834813	18.905255	-0.041286	1.528523
218.398745	595.988922	18.910259	-0.041303	1.521284
218.264462	588.186248	18.915264	-0.041273	1.514010
218.115049	580.376252	18.920269	-0.041241	1.506693
217.949300	572.570611	18.925274	-0.041205	1.499341
218.216966	564.703951	18.930279	-0.041250	1.491962
217.940329	556.925440	18.935283	-0.041193	1.484546
217.756680	549.143826	18.940288	-0.041154	1.477104
217.641057	541.309573	18.945293	-0.041127	1.469585
217.599022	533.479588	18.950298	-0.041115	1.462042
217.661087	525.668173	18.955303	-0.041121	1.454495
217.580434	517.865052	18.960307	-0.041101	1.446894
217.596056	510.059193	18.965312	-0.041099	1.439266
217.496174	502.289563	18.970317	-0.041076	1.431614
217.349334	494.504330	18.975322	-0.041043	1.423897
217.387974	486.712681	18.980327	-0.041045	1.416163
217.285354	478.939439	18.985331	-0.041021	1.408381
217.119173	471.170888	18.990336	-0.040986	1.400550
217.089714	463.404395	18.995341	-0.040975	1.392700
216.984714	455.607426	19.000346	-0.040951	1.384761
216.868986	447.855437	19.005351	-0.040924	1.376821
216.997332	440.048034	19.010355	-0.040943	1.368820
216.983162	432.277201	19.015360	-0.040935	1.360785
216.888374	424.553024	19.020365	-0.040913	1.352736
216.643099	416.814690	19.025370	-0.040862	1.344599
216.537677	409.067406	19.030375	-0.040838	1.336427
216.473694	401.321771	19.035379	-0.040821	1.328213
216.490867	393.566789	19.040384	-0.040819	1.319954
216.482281	385.776182	19.045389	-0.040812	1.311599
216.311840	377.986190	19.050394	-0.040776	1.303161
216.191952	370.280990	19.055399	-0.040748	1.294771
216.235996	362.539867	19.060403	-0.040752	1.286316
216.218730	354.830185	19.065408	-0.040744	1.277829
216.144688	347.129190	19.070413	-0.040725	1.269284
215.780481	339.467411	19.075418	-0.040652	1.260670
216.039657	331.721171	19.080423	-0.040695	1.252021
215.926520	324.040821	19.085427	-0.040669	1.243314
215.607293	316.390712	19.090432	-0.040605	1.234541
215.516947	308.692380	19.095437	-0.040583	1.225694
215.519272	301.002932	19.100442	-0.040579	1.216811
215.545739	293.306045	19.105447	-0.040579	1.207859
215.351165	285.670485	19.110451	-0.040538	1.198868
215.169049	278.027453	19.115456	-0.040499	1.189802
215.182542	270.362158	19.120461	-0.040497	1.180681
214.944586	262.740776	19.125466	-0.040448	1.171489
214.925105	255.091362	19.130471	-0.040439	1.162236
215.044337	247.429230	19.135475	-0.040456	1.152922
214.811205	239.792124	19.140480	-0.040408	1.143488
214.855245	232.164066	19.145485	-0.040411	1.134046
214.580699	224.574126	19.150490	-0.040355	1.124505
214.514552	216.982725	19.155495	-0.040338	1.114925
214.526982	209.370493	19.160499	-0.040336	1.105252
214.541960	201.774743	19.165504	-0.040334	1.095516
214.376010	194.217312	19.170509	-0.040298	1.085702
214.246309	186.670004	19.175514	-0.040269	1.075820
214.287636	179.076216	19.180519	-0.040272	1.065824
214.303987	171.526318	19.185523	-0.040270	1.055786
214.056490	164.014909	19.190528	-0.040219	1.045641
213.975845	156.509065	19.195533	-0.040199	1.035445
213.990863	148.973073	19.200538	-0.040197	1.025128
213.777837	141.500821	19.205543	-0.040153	1.014740
213.672857	134.020020	19.210547	-0.040129	1.004258
213.541610	126.544081	19.215552	-0.040099	0.993667
213.531469	119.044333	19.220557	-0.040093	0.982957
213.444204	111.592119	19.225562	-0.040072	0.972179
213.125728	104.199042	19.230567	-0.040008	0.961307
213.259334	96.748704	19.235571	-0.040028	0.950344
213.142215	89.345390	19.240576	-0.040001	0.939257
213.078265	81.957348	19.245581	-0.039985	0.928075
212.922379	74.604592	19.250586	-0.039951	0.916786
212.706374	67.261065	19.255591	-0.039906	0.905354
212.504449	60.176654	19.260595	-0.039864	0.894188