Fri Mar 12 12:44:37 2021

Number of Points = 3628
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.805881	-0.229664	0.000000	-0.000186	0.716796

0.664141	-0.228073	0.005005	-0.000159	0.716748
0.754798	-0.241581	0.010010	-0.000176	0.716753
0.567887	-0.206473	0.015014	-0.000141	0.716756
0.439042	-0.186519	0.020019	-0.000117	0.716750
0.461009	-0.185820	0.025024	-0.000120	0.716758
0.333983	-0.168319	0.030029	-0.000097	0.716748
0.278514	-0.156112	0.035034	-0.000086	0.716752
0.338901	-0.166436	0.040038	-0.000097	0.716752
0.299278	-0.162572	0.045043	-0.000089	0.716746
0.514262	-0.196648	0.050048	-0.000129	0.716753
0.256804	-0.270664	0.055053	-0.000081	0.716516
0.404574	-0.333246	0.060058	-0.000108	0.716443
0.481659	-0.345362	0.065062	-0.000122	0.716446
0.461045	-0.342991	0.070067	-0.000118	0.716443
0.434339	-0.333978	0.075072	-0.000113	0.716451
0.609267	-0.371168	0.080077	-0.000145	0.716439
0.392725	-0.399546	0.085082	-0.000105	0.716305
0.231723	-0.456752	0.090086	-0.000074	0.716135
-0.189221	-0.388069	0.095091	0.000004	0.716122
-0.171891	-0.385366	0.100096	0.000001	0.716133
-0.477093	-0.335725	0.105101	0.000058	0.716123
-0.396281	-0.346024	0.110106	0.000043	0.716131
0.236628	-0.530732	0.115110	-0.000074	0.715988
0.465048	-0.628053	0.120115	-0.000116	0.715875
0.607665	-0.647867	0.125120	-0.000143	0.715886
0.442476	-0.621551	0.130125	-0.000112	0.715879
0.306846	-0.691374	0.135130	-0.000086	0.715692
0.042421	-0.719100	0.140134	-0.000037	0.715543
-0.218470	-0.676914	0.145139	0.000012	0.715534
-0.153698	-0.682667	0.150144	0.000000	0.715545
-0.245299	-0.751592	0.155149	0.000018	0.715376
-0.265602	-0.822103	0.160154	0.000022	0.715228
-0.214141	-0.830169	0.165158	0.000013	0.715230
-0.302083	-0.817060	0.170163	0.000029	0.715224
-0.448213	-0.914853	0.175168	0.000057	0.714978
-0.405096	-0.963276	0.180173	0.000049	0.714897
-0.130307	-1.011562	0.185178	-0.000002	0.714898
-0.190892	-1.052358	0.190182	0.000010	0.714795
-0.036021	-1.177838	0.195187	-0.000019	0.714600
0.351868	-1.242736	0.200192	-0.000091	0.714608
-0.040083	-1.254778	0.205197	-0.000018	0.714445
-0.802366	-1.207225	0.210202	0.000125	0.714269
-0.936241	-1.181644	0.215206	0.000150	0.714272
-0.682300	-1.280394	0.220211	0.000103	0.714165
-0.524871	-1.407932	0.225216	0.000074	0.713967
-0.749954	-1.372425	0.230221	0.000116	0.713958
-0.625987	-1.462366	0.235226	0.000093	0.713822
-0.830164	-1.514911	0.240230	0.000131	0.713645
-1.046188	-1.480858	0.245235	0.000172	0.713636
-0.903478	-1.591690	0.250240	0.000146	0.713465
-1.311304	-1.578830	0.255245	0.000222	0.713346
-1.278597	-1.582538	0.260250	0.000216	0.713350
-0.810805	-1.800015	0.265254	0.000129	0.713082
-0.725525	-1.850234	0.270259	0.000114	0.713012
-1.024248	-1.847676	0.275264	0.000169	0.712911
-1.487314	-1.871068	0.280269	0.000256	0.712700
-1.232325	-1.913638	0.285274	0.000209	0.712705
-1.386020	-2.013363	0.290278	0.000238	0.712451
-2.029519	-1.935184	0.295283	0.000358	0.712378
-1.884792	-1.979582	0.300288	0.000331	0.712341
-1.350613	-2.203806	0.305293	0.000232	0.712083
-1.380039	-2.197935	0.310298	0.000238	0.712084
-2.021472	-2.214944	0.315302	0.000357	0.711822
-2.375849	-2.186640	0.320307	0.000424	0.711752
-2.290570	-2.236441	0.325312	0.000408	0.711682
-2.701146	-2.279911	0.330317	0.000485	0.711449
-3.369543	-2.161588	0.335322	0.000609	0.711447
-3.036576	-2.306803	0.340326	0.000548	0.711275
-4.233790	-2.167706	0.345331	0.000771	0.711127
-3.951434	-2.212778	0.350336	0.000718	0.711137
-3.905393	-2.293843	0.355341	0.000710	0.710991
-4.943445	-2.170875	0.360346	0.000904	0.710867
-4.807165	-2.193282	0.365350	0.000879	0.710870
-5.004798	-2.196571	0.370355	0.000916	0.710793
-5.212374	-2.290244	0.375360	0.000955	0.710531
-5.351546	-2.269232	0.380365	0.000981	0.710523
-6.220506	-2.113869	0.385370	0.001143	0.710524
-5.788778	-2.284110	0.390374	0.001063	0.710337
-6.722558	-2.183405	0.395379	0.001237	0.710205
-6.794681	-2.166137	0.400384	0.001250	0.710214
-6.917166	-2.147353	0.405389	0.001273	0.710207
-6.808711	-2.216946	0.410394	0.001253	0.710106
-7.457880	-2.209417	0.415398	0.001375	0.709889
-7.642976	-2.180254	0.420403	0.001409	0.709881
-7.665898	-2.170584	0.425408	0.001414	0.709892
-7.613943	-2.183082	0.430413	0.001404	0.709885
-7.899300	-2.231493	0.435418	0.001458	0.709686
-8.539018	-2.164159	0.440422	0.001577	0.709592
-8.406438	-2.191531	0.445427	0.001553	0.709584
-8.364715	-2.194399	0.450432	0.001545	0.709593
-8.505827	-2.173736	0.455437	0.001572	0.709584
-8.289477	-2.327588	0.460442	0.001532	0.709352
-9.340643	-2.186355	0.465446	0.001728	0.709260
-9.630990	-2.137649	0.470451	0.001782	0.709253
-8.890837	-2.265306	0.475456	0.001644	0.709261
-9.065074	-2.237098	0.480461	0.001677	0.709255
-9.637840	-2.216215	0.485466	0.001784	0.709092
-10.402090	-2.148592	0.490470	0.001926	0.708954
-9.882135	-2.245118	0.495475	0.001830	0.708946
-9.975843	-2.224867	0.500480	0.001848	0.708953
-10.559732	-2.122945	0.505485	0.001957	0.708948
-10.420504	-2.147406	0.510490	0.001931	0.708948
-10.080752	-2.285922	0.515494	0.001868	0.708792
-11.672358	-2.084446	0.520499	0.002164	0.708627
-11.053369	-2.189894	0.525504	0.002049	0.708636
-11.028609	-2.195513	0.530509	0.002045	0.708633
-11.502686	-2.110821	0.535514	0.002134	0.708633
-10.846989	-2.226787	0.540518	0.002012	0.708634
-11.181065	-2.199351	0.545523	0.002074	0.708569
-12.076200	-2.149049	0.550528	0.002241	0.708350
-11.908998	-2.181340	0.555533	0.002210	0.708345
-12.122762	-2.143549	0.560538	0.002250	0.708344
-11.564477	-2.240831	0.565542	0.002147	0.708348
-11.994290	-2.167922	0.570547	0.002227	0.708340
-11.953131	-2.171400	0.575552	0.002219	0.708347
-12.056597	-2.308459	0.580557	0.002239	0.708035
-12.991032	-2.157246	0.585562	0.002413	0.708004
-13.212515	-2.113990	0.590566	0.002455	0.708011
-12.636494	-2.219303	0.595571	0.002348	0.708005
-12.530162	-2.235294	0.600576	0.002328	0.708010
-13.110425	-2.134514	0.605581	0.002436	0.708005
-13.061959	-2.212210	0.610586	0.002428	0.707866
-13.712547	-2.181209	0.615590	0.002549	0.707695
-13.785141	-2.173404	0.620595	0.002563	0.707684
-13.813171	-2.161284	0.625600	0.002568	0.707698
-13.794232	-2.168276	0.630605	0.002565	0.707690
-13.842904	-2.158430	0.635610	0.002574	0.707692
-13.859957	-2.151846	0.640614	0.002578	0.707699
-13.829098	-2.239134	0.645619	0.002572	0.707534
-14.578067	-2.182813	0.650624	0.002712	0.707379
-14.575281	-2.186729	0.655629	0.002712	0.707371
-14.617887	-2.179054	0.660634	0.002720	0.707371
-14.317305	-2.229556	0.665638	0.002664	0.707377
-14.769903	-2.154364	0.670643	0.002749	0.707365
-14.882847	-2.129134	0.675648	0.002770	0.707375
-14.670521	-2.276882	0.680653	0.002731	0.707154
-15.640140	-2.145416	0.685658	0.002911	0.707071
-15.857460	-2.103177	0.690662	0.002952	0.707077
-15.466752	-2.177055	0.695667	0.002880	0.707068
-15.025740	-2.249869	0.700672	0.002798	0.707079
-15.431820	-2.182070	0.705677	0.002874	0.707070
-15.540954	-2.163120	0.710682	0.002894	0.707068
-15.739789	-2.286808	0.715686	0.002932	0.706748
-16.265948	-2.195114	0.720691	0.003030	0.706743
-16.558034	-2.138888	0.725696	0.003084	0.706751
-16.144974	-2.216827	0.730701	0.003008	0.706742
-16.206848	-2.203968	0.735706	0.003019	0.706745
-16.360676	-2.174796	0.740710	0.003048	0.706748
-16.603931	-2.170446	0.745715	0.003094	0.706670
-17.107999	-2.191545	0.750720	0.003188	0.706446
-16.958482	-2.220680	0.755725	0.003160	0.706441
-17.442889	-2.135843	0.760730	0.003251	0.706437
-17.076745	-2.198660	0.765734	0.003183	0.706442
-17.227169	-2.176465	0.770739	0.003211	0.706432
-17.304480	-2.159884	0.775744	0.003226	0.706437
-17.007173	-2.268030	0.780749	0.003171	0.706326
-18.050053	-2.183433	0.785754	0.003365	0.706122
-18.186867	-2.157488	0.790758	0.003391	0.706124
-18.436109	-2.117908	0.795763	0.003437	0.706114
-17.971253	-2.196693	0.800768	0.003351	0.706122
-18.182263	-2.160861	0.805773	0.003391	0.706118
-18.593514	-2.087160	0.810778	0.003467	0.706118
-17.928919	-2.228494	0.815782	0.003344	0.706072
-18.727010	-2.195564	0.820787	0.003493	0.705851
-18.930075	-2.156024	0.825792	0.003531	0.705858
-18.708074	-2.197225	0.830797	0.003490	0.705854
-18.498081	-2.234889	0.835802	0.003451	0.705853
-18.617475	-2.210419	0.840806	0.003473	0.705859
-18.805206	-2.181491	0.845811	0.003509	0.705849
-18.992208	-2.284072	0.850816	0.003544	0.705575
-19.953842	-2.141734	0.855821	0.003723	0.705516
-20.077176	-2.120016	0.860826	0.003746	0.705515
-19.382705	-2.241486	0.865830	0.003617	0.705520
-19.724840	-2.183323	0.870835	0.003681	0.705513
-20.084780	-2.114111	0.875840	0.003748	0.705523
-19.736524	-2.179255	0.880845	0.003684	0.705516
-19.989345	-2.276703	0.885850	0.003731	0.705229
-20.715655	-2.156951	0.890854	0.003867	0.705209
-20.968312	-2.115899	0.895859	0.003914	0.705201
-20.242584	-2.241085	0.900864	0.003779	0.705208
-20.462726	-2.204589	0.905869	0.003820	0.705202
-21.019238	-2.105491	0.910874	0.003924	0.705202
-20.418808	-2.225438	0.915878	0.003813	0.705175
-21.174723	-2.240294	0.920883	0.003954	0.704874
-21.681751	-2.145326	0.925888	0.004048	0.704882
-21.817952	-2.120615	0.930893	0.004074	0.704883
-21.503662	-2.178269	0.935898	0.004016	0.704879
-21.421238	-2.189045	0.940902	0.004000	0.704886
-21.860662	-2.115508	0.945907	0.004082	0.704876
-21.466848	-2.181410	0.950912	0.004009	0.704884
-21.889384	-2.244631	0.955917	0.004088	0.704605
-22.811204	-2.091752	0.960922	0.004260	0.704581
-22.318553	-2.177253	0.965926	0.004169	0.704585
-22.240392	-2.193043	0.970931	0.004154	0.704581
-22.689127	-2.109902	0.975936	0.004238	0.704587
-22.374474	-2.168551	0.980941	0.004180	0.704582
-22.259926	-2.189975	0.985946	0.004159	0.704579
-22.894111	-2.223336	0.990950	0.004277	0.704283
-23.613039	-2.112078	0.995955	0.004411	0.704249
-23.369468	-2.151318	1.000960	0.004366	0.704257
-23.062517	-2.208168	1.005965	0.004309	0.704252
-23.745087	-2.086085	1.010970	0.004437	0.704252
-23.285382	-2.165561	1.015974	0.004351	0.704257
-23.031371	-2.214173	1.020979	0.004304	0.704250
-23.586795	-2.237932	1.025984	0.004408	0.704002
-24.424872	-2.115833	1.030989	0.004564	0.703946
-24.238208	-2.150850	1.035994	0.004530	0.703942
-23.893305	-2.206958	1.040998	0.004466	0.703953
-24.327504	-2.136547	1.046003	0.004547	0.703938
-24.256022	-2.142553	1.051008	0.004534	0.703951
-23.648761	-2.254067	1.056013	0.004421	0.703944
-24.831806	-2.197938	1.061018	0.004641	0.703631
-24.822541	-2.197381	1.066022	0.004640	0.703635
-25.081149	-2.156259	1.071027	0.004688	0.703625
-25.070318	-2.154047	1.076032	0.004687	0.703633
-24.955024	-2.175334	1.081037	0.004665	0.703631
-24.805111	-2.203334	1.086042	0.004638	0.703628
-24.629752	-2.274937	1.091046	0.004605	0.703546
-26.108755	-2.117269	1.096051	0.004881	0.703331
-25.642449	-2.197505	1.101056	0.004794	0.703337
-25.402777	-2.241586	1.106061	0.004750	0.703333
-26.134518	-2.111426	1.111066	0.004886	0.703332
-25.669005	-2.190592	1.116070	0.004800	0.703340
-25.630336	-2.202934	1.121075	0.004793	0.703328
-25.633467	-2.308719	1.126080	0.004794	0.703113
-26.923854	-2.134719	1.131085	0.005034	0.702999
-26.867336	-2.145603	1.136090	0.005024	0.702997
-26.122139	-2.275452	1.141094	0.004886	0.703003
-26.814283	-2.155711	1.146099	0.005015	0.702995
-26.717643	-2.168532	1.151104	0.004997	0.703003
-26.544289	-2.201214	1.156109	0.004965	0.702999
-27.286457	-2.208474	1.161114	0.005103	0.702717
-27.572814	-2.171395	1.166118	0.005157	0.702688
-27.618021	-2.167231	1.171123	0.005166	0.702680
-27.338079	-2.214205	1.176128	0.005114	0.702685
-27.650737	-2.159071	1.181133	0.005172	0.702683
-27.890106	-2.117661	1.186138	0.005217	0.702680
-27.519598	-2.180281	1.191142	0.005148	0.702687
-28.108500	-2.194492	1.196147	0.005258	0.702445
-29.123048	-2.052313	1.201152	0.005447	0.702367
-28.416296	-2.182304	1.206157	0.005316	0.702358
-28.279500	-2.208351	1.211162	0.005291	0.702354
-28.809263	-2.107322	1.216166	0.005390	0.702367
-28.582662	-2.152162	1.221171	0.005348	0.702358
-28.244823	-2.209926	1.226176	0.005285	0.702362
-28.678850	-2.183065	1.231181	0.005366	0.702260
-29.808523	-2.080319	1.236186	0.005577	0.702060
-28.860514	-2.243913	1.241190	0.005400	0.702070
-29.395027	-2.152149	1.246195	0.005500	0.702062
-29.453874	-2.139374	1.251200	0.005511	0.702067
-29.144662	-2.195663	1.256205	0.005454	0.702064
-29.469482	-2.137932	1.261210	0.005515	0.702063
-29.441633	-2.212195	1.266214	0.005510	0.701922
-30.263351	-2.160644	1.271219	0.005663	0.701730
-30.007878	-2.201141	1.276224	0.005616	0.701739
-30.145949	-2.178136	1.281229	0.005642	0.701736
-30.326526	-2.146934	1.286234	0.005676	0.701733
-29.954906	-2.209877	1.291238	0.005607	0.701739
-30.022672	-2.203343	1.296243	0.005620	0.701728
-30.549340	-2.218526	1.301248	0.005718	0.701506
-31.218252	-2.138415	1.306253	0.005843	0.701427
-31.156887	-2.150432	1.311258	0.005831	0.701424
-30.960677	-2.179131	1.316262	0.005795	0.701436
-31.158112	-2.149047	1.321267	0.005832	0.701425
-30.908216	-2.190403	1.326272	0.005786	0.701431
-31.179491	-2.141562	1.331277	0.005837	0.701432
-31.699071	-2.159230	1.336282	0.005934	0.701208
-31.990834	-2.151286	1.341286	0.005988	0.701118
-31.936121	-2.164968	1.346291	0.005978	0.701110
-31.686111	-2.207040	1.351296	0.005932	0.701114
-31.977850	-2.153740	1.356301	0.005987	0.701117
-31.910092	-2.166896	1.361306	0.005974	0.701114
-31.697625	-2.201195	1.366310	0.005935	0.701121
-32.197583	-2.222271	1.371315	0.006028	0.700897
-32.526603	-2.176229	1.376320	0.006090	0.700871
-32.550415	-2.172324	1.381325	0.006094	0.700870
-32.597388	-2.166176	1.386330	0.006103	0.700865
-32.311528	-2.213256	1.391334	0.006050	0.700872
-32.671085	-2.151329	1.396339	0.006118	0.700867
-32.819102	-2.224647	1.401344	0.006145	0.700665
-33.607070	-2.150818	1.406349	0.006292	0.700529
-33.198388	-2.225155	1.411354	0.006217	0.700526
-33.307493	-2.201342	1.416358	0.006237	0.700534
-33.628288	-2.149482	1.421363	0.006297	0.700523
-33.218336	-2.218117	1.426368	0.006221	0.700531
-33.295605	-2.229473	1.431373	0.006236	0.700480
-34.562909	-2.137419	1.436378	0.006472	0.700208
-34.104676	-2.214591	1.441382	0.006387	0.700216
-34.331532	-2.178940	1.446387	0.006429	0.700206
-34.157609	-2.205871	1.451392	0.006397	0.700214
-33.936538	-2.245252	1.456397	0.006356	0.700214
-34.219930	-2.196401	1.461402	0.006409	0.700210
-34.390328	-2.265706	1.466406	0.006441	0.700007
-35.252017	-2.173234	1.471411	0.006602	0.699882
-35.076402	-2.201124	1.476416	0.006569	0.699889
-34.898636	-2.233051	1.481421	0.006537	0.699888
-35.279261	-2.168128	1.486426	0.006608	0.699881
-34.689458	-2.268383	1.491430	0.006498	0.699891
-35.082677	-2.220561	1.496435	0.006572	0.699845
-36.180374	-2.148583	1.501440	0.006776	0.699593
-35.713509	-2.233376	1.506445	0.006690	0.699590
-35.918051	-2.199469	1.511450	0.006728	0.699584
-35.916059	-2.195281	1.516454	0.006728	0.699593
-36.023383	-2.180480	1.521459	0.006748	0.699584
-35.719804	-2.232192	1.526464	0.006692	0.699588
-35.815654	-2.295787	1.531469	0.006710	0.699424
-37.417094	-2.094498	1.536474	0.007008	0.699252
-36.613918	-2.232470	1.541478	0.006859	0.699262
-36.825163	-2.199632	1.546483	0.006899	0.699252
-37.101475	-2.146889	1.551488	0.006950	0.699259
-36.713102	-2.216070	1.556493	0.006878	0.699258
-36.888257	-2.187478	1.561498	0.006911	0.699252
-36.844143	-2.268117	1.566502	0.006903	0.699104
-37.757814	-2.183836	1.571507	0.007073	0.698944
-37.595411	-2.209030	1.576512	0.007043	0.698951
-37.574146	-2.213508	1.581517	0.007040	0.698949
-38.013369	-2.137549	1.586522	0.007122	0.698944
-37.576369	-2.209566	1.591526	0.007041	0.698955
-37.639921	-2.202643	1.596531	0.007053	0.698946
-38.272678	-2.199624	1.601536	0.007171	0.698722
-38.843520	-2.142845	1.606541	0.007277	0.698630
-38.487768	-2.207210	1.611546	0.007211	0.698628
-38.462929	-2.207180	1.616550	0.007207	0.698636
-38.980359	-2.120380	1.621555	0.007303	0.698625
-38.524388	-2.198856	1.626560	0.007219	0.698630
-38.054725	-2.282117	1.631565	0.007132	0.698631
-39.113176	-2.195673	1.636570	0.007329	0.698422
-39.655912	-2.135519	1.641574	0.007430	0.698347
-39.371830	-2.191170	1.646579	0.007378	0.698336
-39.350775	-2.191657	1.651584	0.007374	0.698343
-39.670837	-2.131879	1.656589	0.007434	0.698348
-39.574287	-2.152547	1.661594	0.007416	0.698340
-39.232554	-2.208618	1.666598	0.007353	0.698350
-39.889750	-2.202786	1.671603	0.007475	0.698123
-40.565123	-2.138557	1.676608	0.007601	0.698008
-39.672042	-2.296806	1.681613	0.007435	0.698009
-40.282383	-2.189895	1.686618	0.007549	0.698005
-40.363883	-2.171171	1.691622	0.007565	0.698013
-40.236871	-2.197578	1.696627	0.007541	0.698005
-40.319273	-2.181340	1.701632	0.007557	0.698007
-40.861205	-2.232931	1.706637	0.007658	0.697705
-41.088271	-2.199172	1.711642	0.007700	0.697691
-40.907857	-2.228086	1.716646	0.007667	0.697697
-41.363771	-2.149483	1.721651	0.007752	0.697691
-41.328201	-2.154173	1.726656	0.007746	0.697694
-40.865772	-2.236417	1.731661	0.007660	0.697694
-41.103230	-2.231052	1.736666	0.007705	0.697618
-42.084405	-2.175660	1.741670	0.007887	0.697374
-41.643894	-2.258940	1.746675	0.007806	0.697364
-41.754004	-2.236036	1.751680	0.007826	0.697370
-41.987383	-2.191106	1.756685	0.007870	0.697377
-41.942538	-2.203467	1.761690	0.007862	0.697367
-41.746476	-2.236554	1.766694	0.007826	0.697371
-42.290627	-2.236311	1.771699	0.007927	0.697173
-43.056770	-2.149905	1.776704	0.008070	0.697070
-42.631015	-2.221973	1.781709	0.007991	0.697077
-42.739664	-2.204808	1.786714	0.008012	0.697072
-42.927751	-2.167881	1.791718	0.008047	0.697079
-42.677684	-2.216808	1.796723	0.008001	0.697070
-42.550639	-2.237432	1.801728	0.007977	0.697073
-43.374456	-2.237610	1.806733	0.008131	0.696773
-43.953080	-2.150432	1.811738	0.008239	0.696740
-43.287812	-2.264001	1.816742	0.008115	0.696750
-43.717826	-2.190200	1.821747	0.008196	0.696743
-43.887294	-2.158357	1.826752	0.008227	0.696746
-43.706110	-2.190094	1.831757	0.008194	0.696747
-43.799321	-2.175146	1.836762	0.008211	0.696743
-44.139724	-2.246973	1.841766	0.008275	0.696472
-44.483947	-2.204239	1.846771	0.008339	0.696433
-44.302585	-2.234555	1.851776	0.008306	0.696437
-44.157682	-2.258444	1.856781	0.008279	0.696441
-44.816689	-2.143065	1.861786	0.008402	0.696436
-44.259021	-2.238938	1.866790	0.008299	0.696443
-44.387960	-2.278378	1.871795	0.008323	0.696315
-45.520363	-2.170860	1.876800	0.008534	0.696122
-45.089912	-2.244846	1.881805	0.008454	0.696127
-45.306283	-2.210641	1.886810	0.008495	0.696117
-45.364325	-2.195346	1.891814	0.008506	0.696127
-45.055479	-2.254410	1.896819	0.008448	0.696118
-45.102066	-2.242689	1.901824	0.008457	0.696125
-45.571665	-2.265994	1.906829	0.008545	0.695906
-46.093424	-2.192604	1.911834	0.008642	0.695865
-45.934721	-2.214293	1.916838	0.008613	0.695878
-45.882597	-2.227407	1.921843	0.008604	0.695870
-46.230731	-2.163616	1.926848	0.008669	0.695873
-46.006111	-2.202798	1.931853	0.008627	0.695874
-45.921665	-2.294355	1.936858	0.008612	0.695718
-47.114755	-2.168925	1.941862	0.008834	0.695539
-46.800010	-2.229498	1.946867	0.008776	0.695529
-46.900804	-2.209256	1.951872	0.008795	0.695533
-46.680598	-2.246773	1.956877	0.008754	0.695536
-46.820018	-2.225678	1.961882	0.008780	0.695528
-46.697591	-2.242275	1.966886	0.008758	0.695538
-47.338835	-2.282652	1.971891	0.008877	0.695222
-47.836929	-2.196308	1.976896	0.008970	0.695216
-47.753653	-2.208330	1.981901	0.008955	0.695221
-47.686225	-2.224248	1.986906	0.008943	0.695213
-47.582028	-2.236755	1.991910	0.008923	0.695225
-47.587868	-2.240290	1.996915	0.008925	0.695215
-48.060976	-2.268341	2.001920	0.009013	0.694985

-48.640221	-2.207236	2.011917	0.009121	0.694897
-48.733098	-2.190080	2.021914	0.009139	0.694898
-48.373960	-2.255398	2.031910	0.009073	0.694894
-48.586354	-2.214359	2.041907	0.009113	0.694900
-48.454260	-2.236420	2.051904	0.009089	0.694902
-48.702053	-2.193653	2.061901	0.009135	0.694898
-48.590352	-2.212611	2.071898	0.009115	0.694899
-48.511628	-2.226871	2.081894	0.009101	0.694897
-48.497434	-2.228281	2.091891	0.009099	0.694899
-48.318408	-2.260587	2.101888	0.009066	0.694897
-48.572473	-2.215364	2.111885	0.009114	0.694896
-48.610277	-2.208912	2.121882	0.009121	0.694894
-47.836712	-2.188866	2.131878	0.008978	0.695216
-47.914956	-2.172256	2.141875	0.008993	0.695221
-47.571206	-2.232992	2.151872	0.008929	0.695221
-48.026224	-2.153030	2.161869	0.009014	0.695218
-47.593695	-2.231668	2.171866	0.008934	0.695214
-47.031695	-2.195307	2.181862	0.008830	0.695492
-46.815487	-2.213851	2.191859	0.008791	0.695532
-46.691825	-2.234674	2.201856	0.008768	0.695533
-47.200322	-2.145519	2.211853	0.008863	0.695529
-46.461713	-2.188596	2.221850	0.008726	0.695709
-45.890716	-2.211893	2.231846	0.008620	0.695869
-45.967280	-2.197533	2.241843	0.008635	0.695869
-45.900526	-2.207514	2.251840	0.008623	0.695872
-45.665459	-2.178945	2.261837	0.008580	0.696015
-45.139324	-2.219480	2.271834	0.008482	0.696123
-45.321397	-2.186873	2.281830	0.008517	0.696122
-45.249999	-2.199022	2.291827	0.008504	0.696122
-44.402493	-2.197535	2.301824	0.008347	0.696433
-44.445594	-2.186462	2.311821	0.008355	0.696439
-44.188175	-2.231602	2.321818	0.008308	0.696439
-44.203296	-2.172562	2.331814	0.008311	0.696553
-43.254498	-2.245473	2.341811	0.008135	0.696749
-43.500475	-2.202504	2.351808	0.008181	0.696746
-43.632893	-2.177032	2.361805	0.008206	0.696749
-42.610547	-2.219928	2.371802	0.008016	0.697032
-42.577707	-2.203146	2.381798	0.008011	0.697077
-42.353180	-2.241534	2.391795	0.007970	0.697080
-42.542916	-2.179910	2.401792	0.008005	0.697135
-41.961992	-2.167084	2.411789	0.007898	0.697372
-41.583620	-2.234294	2.421786	0.007828	0.697371
-41.866980	-2.183317	2.431782	0.007881	0.697371
-41.101510	-2.186822	2.441779	0.007739	0.697641
-40.941505	-2.188325	2.451776	0.007710	0.697695
-40.718232	-2.228253	2.461773	0.007669	0.697694
-40.821819	-2.158282	2.471770	0.007688	0.697798
-39.982561	-2.204357	2.481766	0.007533	0.698008
-39.815821	-2.233855	2.491763	0.007502	0.698007
-40.012205	-2.197203	2.501760	0.007539	0.698010
-39.228356	-2.198013	2.511757	0.007394	0.698291
-39.146257	-2.185440	2.521754	0.007379	0.698346
-39.034673	-2.206714	2.531750	0.007359	0.698342
-38.797359	-2.216711	2.541747	0.007315	0.698407
-38.293980	-2.195245	2.551744	0.007222	0.698632
-38.095890	-2.229449	2.561741	0.007185	0.698633
-38.527405	-2.153207	2.571738	0.007266	0.698631
-37.588898	-2.182311	2.581734	0.007092	0.698911
-37.296080	-2.214333	2.591731	0.007038	0.698951
-37.332413	-2.206727	2.601728	0.007045	0.698953
-37.065236	-2.206902	2.611725	0.006996	0.699048
-36.446819	-2.213115	2.621722	0.006881	0.699259
-36.434877	-2.213695	2.631718	0.006879	0.699261
-36.265914	-2.243241	2.641715	0.006848	0.699261
-36.080274	-2.154877	2.651712	0.006814	0.699507
-35.479582	-2.221267	2.661709	0.006703	0.699588
-35.740861	-2.174275	2.671706	0.006752	0.699588
-35.358011	-2.197728	2.681702	0.006681	0.699678
-34.515176	-2.242821	2.691699	0.006525	0.699891
-34.682216	-2.212867	2.701696	0.006556	0.699890
-34.669809	-2.214954	2.711693	0.006555	0.699890
-34.124872	-2.189818	2.721690	0.006454	0.700137
-33.865657	-2.197465	2.731686	0.006406	0.700214
-33.689468	-2.226833	2.741683	0.006374	0.700217
-33.868046	-2.152780	2.751680	0.006407	0.700302
-32.878856	-2.216929	2.761677	0.006224	0.700528
-33.035730	-2.188944	2.771674	0.006253	0.700528
-32.798147	-2.230994	2.781670	0.006210	0.700527
-32.176175	-2.212957	2.791667	0.006094	0.700788
-32.182960	-2.171124	2.801664	0.006096	0.700869
-31.962084	-2.210117	2.811661	0.006055	0.700869
-32.215426	-2.133455	2.821658	0.006103	0.700932
-31.480950	-2.174297	2.831654	0.005967	0.701113
-31.262932	-2.209924	2.841651	0.005927	0.701119
-31.456667	-2.163599	2.851648	0.005963	0.701142
-30.557243	-2.180477	2.861645	0.005796	0.701431
-30.558601	-2.180998	2.871642	0.005797	0.701429
-30.314656	-2.223138	2.881638	0.005752	0.701431
-30.154256	-2.144627	2.891635	0.005723	0.701647
-29.788857	-2.164320	2.901632	0.005655	0.701738
-29.556852	-2.205373	2.911629	0.005613	0.701737
-29.577076	-2.133043	2.921626	0.005617	0.701875
-28.509567	-2.229656	2.931622	0.005418	0.702064
-28.831844	-2.170636	2.941619	0.005479	0.702066
-28.629704	-2.204083	2.951616	0.005442	0.702071
-28.130262	-2.155888	2.961613	0.005349	0.702347
-28.053585	-2.162439	2.971610	0.005336	0.702361
-27.640171	-2.233980	2.981606	0.005259	0.702364
-27.693300	-2.136348	2.991603	0.005269	0.702541
-26.965650	-2.192103	3.001600	0.005134	0.702690
-27.131726	-2.163180	3.011597	0.005166	0.702687
-27.115624	-2.140709	3.021594	0.005163	0.702738
-26.309278	-2.153790	3.031590	0.005014	0.703001
-26.250959	-2.163329	3.041587	0.005003	0.703002
-26.110736	-2.186504	3.051584	0.004978	0.703004
-25.422643	-2.173337	3.061581	0.004850	0.703278
-25.246152	-2.174640	3.071578	0.004818	0.703338
-25.187113	-2.184694	3.081574	0.004807	0.703338
-25.205229	-2.157376	3.091571	0.004811	0.703385
-24.374973	-2.183225	3.101568	0.004657	0.703631
-24.266590	-2.202309	3.111565	0.004637	0.703630
-24.433797	-2.173381	3.121562	0.004669	0.703628
-23.868681	-2.176513	3.131558	0.004564	0.703824
-23.494450	-2.181932	3.141555	0.004495	0.703946
-23.486750	-2.181554	3.151552	0.004494	0.703949
-23.637567	-2.126952	3.161549	0.004523	0.704004
-22.597380	-2.187707	3.171546	0.004329	0.704254
-22.617604	-2.184715	3.181542	0.004334	0.704252
-22.600835	-2.185100	3.191539	0.004331	0.704256
-21.964118	-2.198033	3.201536	0.004213	0.704458
-21.628121	-2.196419	3.211533	0.004151	0.704581
-21.658173	-2.190512	3.221530	0.004157	0.704581
-21.458663	-2.225647	3.231526	0.004120	0.704581
-21.012080	-2.178753	3.241523	0.004038	0.704835
-20.557975	-2.235064	3.251520	0.003954	0.704884
-20.842635	-2.185552	3.261517	0.004007	0.704880
-20.728248	-2.168219	3.271514	0.003986	0.704956
-20.034214	-2.168823	3.281510	0.003858	0.705202
-19.697284	-2.225038	3.291507	0.003795	0.705209
-19.869066	-2.194836	3.301504	0.003828	0.705207
-19.258251	-2.181876	3.311501	0.003715	0.705452
-19.090027	-2.176594	3.321498	0.003684	0.705522
-19.010136	-2.191529	3.331494	0.003669	0.705519
-19.034323	-2.138348	3.341491	0.003674	0.705617
-17.869070	-2.223177	3.351488	0.003458	0.705863
-18.070736	-2.189320	3.361485	0.003496	0.705858
-17.905534	-2.217987	3.371482	0.003466	0.705859
-17.826740	-2.154922	3.381478	0.003451	0.706013
-17.058912	-2.236438	3.391475	0.003309	0.706123
-17.364495	-2.181143	3.401472	0.003366	0.706124
-17.382045	-2.150523	3.411469	0.003370	0.706178
-16.456502	-2.185823	3.421466	0.003198	0.706438
-16.533543	-2.171734	3.431462	0.003213	0.706437
-16.409459	-2.193109	3.441459	0.003191	0.706438
-15.901218	-2.155603	3.451456	0.003096	0.706694
-15.851442	-2.139569	3.461453	0.003088	0.706743
-15.630464	-2.179733	3.471450	0.003047	0.706741
-15.357546	-2.135680	3.481446	0.002997	0.706926
-14.753276	-2.168611	3.491443	0.002885	0.707075
-14.880890	-2.145081	3.501440	0.002909	0.707076
-14.637163	-2.162476	3.511437	0.002864	0.707127
-13.772264	-2.195224	3.521434	0.002703	0.707370
-13.825919	-2.184954	3.531430	0.002714	0.707371
-13.863295	-2.177431	3.541427	0.002721	0.707371
-13.539758	-2.126340	3.551424	0.002662	0.707589
-13.080684	-2.154862	3.561421	0.002577	0.707695
-12.775875	-2.209109	3.571418	0.002520	0.707694
-12.891859	-2.165520	3.581414	0.002542	0.707739
-11.979896	-2.193013	3.591411	0.002373	0.708009
-12.084026	-2.172968	3.601408	0.002393	0.708011
-12.056063	-2.177090	3.611405	0.002388	0.708011
-11.687450	-2.149331	3.621402	0.002320	0.708198
-11.006215	-2.197508	3.631398	0.002194	0.708344
-10.746074	-2.241997	3.641395	0.002146	0.708347
-11.040739	-2.187368	3.651392	0.002201	0.708350
-10.357045	-2.207447	3.661389	0.002074	0.708553
-10.228707	-2.188842	3.671386	0.002051	0.708635
-10.167284	-2.198888	3.681382	0.002040	0.708636
-9.994097	-2.222377	3.691379	0.002008	0.708650
-9.333599	-2.188816	3.701376	0.001886	0.708952
-9.250032	-2.202808	3.711373	0.001871	0.708952
-9.320524	-2.190085	3.721370	0.001884	0.708952
-9.198648	-2.139069	3.731366	0.001862	0.709096
-8.177687	-2.238862	3.741363	0.001673	0.709260
-8.401138	-2.196730	3.751360	0.001715	0.709264
-8.335462	-2.209682	3.761357	0.001703	0.709260
-7.578330	-2.189959	3.771354	0.001562	0.709569
-7.335962	-2.222093	3.781350	0.001518	0.709590
-7.385648	-2.212258	3.791347	0.001528	0.709591
-7.422475	-2.168647	3.801344	0.001535	0.709664
-6.429215	-2.232859	3.811341	0.001351	0.709889
-6.496914	-2.219892	3.821338	0.001364	0.709889
-6.555044	-2.208122	3.831334	0.001375	0.709891
-5.997456	-2.205874	3.841331	0.001272	0.710093
-5.535208	-2.227711	3.851328	0.001186	0.710214
-5.617732	-2.211829	3.861325	0.001202	0.710215
-5.908642	-2.152826	3.871322	0.001256	0.710228
-4.906409	-2.180779	3.881318	0.001070	0.710528
-4.607075	-2.232476	3.891315	0.001015	0.710531
-4.642737	-2.225728	3.901312	0.001022	0.710530
-4.507232	-2.176656	3.911309	0.000998	0.710676
-3.903145	-2.187504	3.921306	0.000886	0.710868
-4.082595	-2.155837	3.931302	0.000919	0.710867
-3.851810	-2.194730	3.941299	0.000877	0.710870
-4.045411	-2.029528	3.951296	0.000913	0.711130
-3.150367	-2.184361	3.961293	0.000747	0.711138
-3.004020	-2.211495	3.971290	0.000721	0.711135
-2.678550	-2.133606	3.981286	0.000660	0.711405
-2.474119	-2.147113	3.991283	0.000623	0.711450
-3.587665	-1.944844	4.001280	0.000831	0.711457
-2.114625	-2.056368	4.011277	0.000557	0.711757
-2.371016	-2.009857	4.021274	0.000605	0.711758
-2.706314	-1.881388	4.031270	0.000668	0.711894
-1.841435	-1.938528	4.041267	0.000507	0.712086
-1.918146	-1.924112	4.051264	0.000522	0.712087
-0.640188	-2.017321	4.061261	0.000285	0.712354
-2.056215	-1.750100	4.071258	0.000549	0.712382
-1.777873	-1.718198	4.081254	0.000497	0.712544
-2.216848	-1.557170	4.091251	0.000580	0.712708
-1.488307	-1.571091	4.101248	0.000444	0.712938
-1.331890	-1.556473	4.111245	0.000416	0.713021
-1.230847	-1.433787	4.121242	0.000397	0.713300
-0.812175	-1.478249	4.131238	0.000320	0.713359
-0.735518	-1.348202	4.141235	0.000306	0.713644
-1.644454	-1.124351	4.151232	0.000476	0.713766
-1.448715	-1.059876	4.161229	0.000440	0.713963
-1.217236	-0.945726	4.171226	0.000397	0.714271
-0.244624	-1.023913	4.181222	0.000216	0.714459
-0.647233	-0.867261	4.191219	0.000292	0.714626
-0.858435	-0.690990	4.201216	0.000331	0.714901
-0.531908	-0.619089	4.211213	0.000271	0.715158
-0.650919	-0.485657	4.221210	0.000294	0.715379
-0.462975	-0.391146	4.231206	0.000259	0.715632
-0.266850	-0.292646	4.241203	0.000223	0.715896
0.061151	-0.232496	4.251200	0.000162	0.716130
0.101863	-0.107992	4.261197	0.000155	0.716390
-0.383141	0.111273	4.271194	0.000246	0.716652
0.000000	0.212198	4.281190	0.000175	0.716986

-0.057040	0.865017	4.286195	0.000185	0.718257
0.226566	2.061656	4.291200	0.000132	0.720716
1.314271	3.703633	4.296205	-0.000071	0.724320
3.178003	5.785579	4.301210	-0.000419	0.729033
4.732020	8.452728	4.306214	-0.000710	0.734739
6.158503	11.632870	4.311219	-0.000978	0.741339
7.742994	15.260158	4.316224	-0.001275	0.748782
9.268231	19.316237	4.321229	-0.001561	0.756935
11.405052	23.668731	4.326234	-0.001962	0.765752
14.270965	28.302266	4.331238	-0.002498	0.775218
17.432980	33.249489	4.336243	-0.003090	0.785231
20.213193	38.637770	4.341248	-0.003611	0.795782
22.250315	44.461448	4.346253	-0.003994	0.806728
24.539912	50.550339	4.351258	-0.004424	0.818063
27.494252	56.815333	4.356262	-0.004978	0.829744
29.735902	63.461225	4.361267	-0.005399	0.841692
30.766997	70.550324	4.366272	-0.005595	0.853852
32.112604	77.772844	4.371277	-0.005850	0.866150
33.108413	85.246291	4.376282	-0.006041	0.878581
34.069110	92.861323	4.381286	-0.006224	0.891053
34.969023	100.637260	4.386291	-0.006397	0.903588
36.292572	108.499478	4.391296	-0.006648	0.916200
37.469856	116.475595	4.396301	-0.006872	0.928774
38.036555	124.680348	4.401306	-0.006983	0.941363
39.001707	132.908647	4.406310	-0.007167	0.953924
39.887473	141.213076	4.411315	-0.007338	0.966413
40.871385	149.590579	4.416320	-0.007526	0.978872
41.551784	158.085345	4.421325	-0.007658	0.991267
42.510294	166.567349	4.426330	-0.007842	1.003558
43.009571	175.175603	4.431334	-0.007940	1.015764
43.529507	183.787071	4.436339	-0.008042	1.027835
44.692434	192.342431	4.441344	-0.008264	1.039840
45.352661	200.989873	4.446349	-0.008392	1.051715
46.314746	209.614394	4.451354	-0.008577	1.063496
47.193523	218.275438	4.456358	-0.008746	1.075176
47.700445	226.973969	4.461363	-0.008846	1.086696
48.874571	235.588599	4.466368	-0.009070	1.098134
49.526389	244.283262	4.471373	-0.009197	1.109442
50.265069	252.966481	4.476378	-0.009339	1.120639
51.312193	261.598861	4.481382	-0.009540	1.131728
51.957478	270.286952	4.486387	-0.009665	1.142692
52.581070	279.013678	4.491392	-0.009787	1.153595
53.092618	287.685182	4.496397	-0.009888	1.164304
53.858830	296.310237	4.501402	-0.010036	1.174912
54.805332	304.893011	4.506406	-0.010217	1.185411
55.238774	313.562602	4.511411	-0.010303	1.195817
56.391622	322.082236	4.516416	-0.010523	1.206101
57.261791	330.662652	4.521421	-0.010691	1.216311
57.505479	339.323494	4.526426	-0.010741	1.226406
58.471771	347.873619	4.531430	-0.010927	1.236433
58.850761	356.454677	4.536435	-0.011003	1.246300
59.314950	365.037974	4.541440	-0.011094	1.256108
59.764167	373.567083	4.546445	-0.011183	1.265777
60.473684	382.067036	4.551450	-0.011321	1.275388
61.092730	390.547719	4.556454	-0.011441	1.284890
61.699168	399.039031	4.561459	-0.011559	1.294330
62.294149	407.512697	4.566464	-0.011676	1.303681
62.914023	416.063907	4.571469	-0.011796	1.313052
63.925990	424.460926	4.576474	-0.011990	1.322263
65.032473	432.808025	4.581478	-0.012201	1.331373
65.811916	441.197593	4.586483	-0.012352	1.340407
66.814922	449.561382	4.591488	-0.012543	1.349393
67.192569	458.012518	4.596493	-0.012619	1.358302
67.831825	466.393998	4.601498	-0.012743	1.367125
68.345588	474.810498	4.606502	-0.012844	1.375905
68.849222	483.199259	4.611507	-0.012943	1.384600
69.860728	491.534582	4.616512	-0.013137	1.393272
70.357769	499.903653	4.621517	-0.013235	1.401837
70.760199	508.290664	4.626522	-0.013315	1.410353
71.297035	516.644114	4.631526	-0.013420	1.418806
71.901616	524.954630	4.636531	-0.013538	1.427177
72.509506	533.305948	4.641536	-0.013656	1.435540
72.964014	541.623013	4.646541	-0.013746	1.443796
73.767531	549.905835	4.651546	-0.013901	1.452027
73.983999	558.278442	4.656550	-0.013946	1.460205
74.574288	566.573239	4.661555	-0.014061	1.468322
74.924409	574.951902	4.666560	-0.014131	1.476436
75.211328	583.240301	4.671565	-0.014190	1.484410
75.707159	591.521130	4.676570	-0.014288	1.492367
76.522292	599.735510	4.681574	-0.014444	1.500267
77.220316	607.978667	4.686579	-0.014580	1.508135
77.752248	616.263484	4.691584	-0.014684	1.515976
78.140419	624.523287	4.696589	-0.014761	1.523730
78.559601	632.800257	4.701594	-0.014844	1.531466
79.167187	641.039877	4.706598	-0.014963	1.539157
79.484148	649.308113	4.711603	-0.015027	1.546793
80.097583	657.564674	4.716608	-0.015146	1.554423
80.279083	665.825892	4.721613	-0.015185	1.561957
80.615555	674.077158	4.726618	-0.015253	1.569469
81.096363	682.312619	4.731622	-0.015347	1.576951
81.747942	690.485373	4.736627	-0.015474	1.584367
82.112904	698.747922	4.741632	-0.015547	1.591786
82.594242	706.964865	4.746637	-0.015642	1.599147
83.186086	715.151353	4.751642	-0.015757	1.606463
84.139759	723.321966	4.756646	-0.015940	1.613783
84.589777	731.534975	4.761651	-0.016029	1.621035
85.344624	739.727954	4.766656	-0.016174	1.628281
85.675616	748.004933	4.771661	-0.016241	1.635508
85.813107	756.242598	4.776666	-0.016272	1.642642
86.136274	764.449589	4.781670	-0.016337	1.649745
86.836904	772.597574	4.786675	-0.016472	1.656818
87.397988	780.769975	4.791680	-0.016582	1.663863
88.082872	788.920060	4.796685	-0.016715	1.670875
88.688040	797.104112	4.801690	-0.016832	1.677876
89.019397	805.306760	4.806694	-0.016899	1.684827
89.319707	813.523032	4.811699	-0.016960	1.691756
89.736282	821.726893	4.816704	-0.017043	1.698662
90.062618	829.902503	4.821709	-0.017109	1.705505
90.455001	838.115271	4.826714	-0.017187	1.712360
90.973497	846.271601	4.831718	-0.017289	1.719156
91.421799	854.406344	4.836723	-0.017377	1.725900
91.762447	862.611501	4.841728	-0.017446	1.732660
92.103095	870.775630	4.846733	-0.017514	1.739361
92.655697	878.905130	4.851738	-0.017622	1.746035
93.274314	887.065860	4.856742	-0.017742	1.752716
93.477711	895.249888	4.861747	-0.017785	1.759339
94.386089	903.343164	4.866752	-0.017959	1.765952
94.663506	911.537448	4.871757	-0.018016	1.772543
94.707433	919.755304	4.876762	-0.018029	1.779098
95.026762	927.911926	4.881766	-0.018094	1.785615
95.581672	936.080122	4.886771	-0.018202	1.792147
95.984261	944.262420	4.891776	-0.018282	1.798647
96.122059	952.406626	4.896781	-0.018313	1.805061
96.720790	960.508118	4.901786	-0.018430	1.811475
97.337948	968.629261	4.906790	-0.018550	1.817883
98.012367	976.707873	4.911795	-0.018680	1.824243
98.487933	984.867156	4.916800	-0.018774	1.830619
98.987967	993.006420	4.921805	-0.018872	1.836960
99.247004	1001.156222	4.926810	-0.018925	1.843259
99.675672	1009.305297	4.931814	-0.019010	1.849556
99.727445	1017.493429	4.936819	-0.019025	1.855817
100.266626	1025.610076	4.941824	-0.019130	1.862059
100.358848	1033.791037	4.946829	-0.019153	1.868277
100.920226	1041.917025	4.951834	-0.019262	1.874488
101.520955	1049.999573	4.956838	-0.019379	1.880649
101.778315	1058.130858	4.961843	-0.019432	1.886787
102.195998	1066.282258	4.966848	-0.019515	1.892939
102.414004	1074.420503	4.971853	-0.019561	1.899038
103.035329	1082.496247	4.976858	-0.019681	1.905116
103.340981	1090.664281	4.981862	-0.019743	1.911208
103.912539	1098.748673	4.986867	-0.019855	1.917249
104.399886	1106.854194	4.991872	-0.019950	1.923276
104.523572	1115.016599	4.996877	-0.019979	1.929286
104.892633	1123.144789	5.001882	-0.020052	1.935280
105.492576	1131.232954	5.006886	-0.020169	1.941251
105.863608	1139.344430	5.011891	-0.020243	1.947195
106.249248	1147.522581	5.016896	-0.020320	1.953171
106.658112	1155.622374	5.021901	-0.020401	1.959074
107.222849	1163.687013	5.026906	-0.020511	1.964952
107.615984	1171.819548	5.031910	-0.020590	1.970841
108.117485	1179.915672	5.036915	-0.020688	1.976699
108.688908	1188.008554	5.041920	-0.020799	1.982544
108.907707	1196.141012	5.046925	-0.020845	1.988363
109.114272	1204.295575	5.051930	-0.020889	1.994179
109.650765	1212.375517	5.056934	-0.020994	1.999960
109.722175	1220.492042	5.061939	-0.021012	2.005702
110.097907	1228.619470	5.066944	-0.021087	2.011466
110.460660	1236.715931	5.071949	-0.021160	2.017191
110.815994	1244.806450	5.076954	-0.021231	2.022894
111.330316	1252.901814	5.081958	-0.021332	2.028601
111.701270	1261.033669	5.086963	-0.021406	2.034303
112.176767	1269.106211	5.091968	-0.021499	2.039958
112.084544	1277.256045	5.096973	-0.021487	2.045593
112.406220	1285.346315	5.101978	-0.021552	2.051213
113.032433	1293.416032	5.106982	-0.021674	2.056835
113.206542	1301.511441	5.111987	-0.021711	2.062413
113.726153	1309.598302	5.116992	-0.021813	2.068005
114.372510	1317.678009	5.121997	-0.021938	2.073589
114.846571	1325.761995	5.127002	-0.022032	2.079144
114.977973	1333.883111	5.132006	-0.022061	2.084675
115.010645	1342.013738	5.137011	-0.022072	2.090189
115.729575	1350.092432	5.142016	-0.022211	2.095720
115.940962	1358.184976	5.147021	-0.022256	2.101196
116.063433	1366.318186	5.152026	-0.022283	2.106677
116.393394	1374.462981	5.157030	-0.022350	2.112171
116.716701	1382.553336	5.162035	-0.022415	2.117613
117.158320	1390.587746	5.167040	-0.022502	2.123016
117.525039	1398.655162	5.172045	-0.022576	2.128420
117.632301	1406.783254	5.177050	-0.022601	2.133825
117.859481	1414.882503	5.182054	-0.022648	2.139209
118.167978	1422.934127	5.187059	-0.022710	2.144556
118.712252	1431.002950	5.192064	-0.022817	2.149923
118.948576	1439.113306	5.197069	-0.022866	2.155275
119.509217	1447.150272	5.202074	-0.022975	2.160595
119.806605	1455.246919	5.207078	-0.023036	2.165917
120.143164	1463.331065	5.212083	-0.023103	2.171222
120.573919	1471.434105	5.217088	-0.023189	2.176534
120.797053	1479.519810	5.222093	-0.023235	2.181803
121.320666	1487.578542	5.227098	-0.023338	2.187069
121.488873	1495.721198	5.232102	-0.023374	2.192344
121.538716	1503.830004	5.237107	-0.023388	2.197574
121.955001	1511.881164	5.242112	-0.023471	2.202787
121.999259	1519.978330	5.247117	-0.023484	2.207984
122.284136	1528.060258	5.252122	-0.023542	2.213181
122.715847	1536.120438	5.257126	-0.023628	2.218365
122.873102	1544.186547	5.262131	-0.023662	2.223516
123.388195	1552.240998	5.267136	-0.023763	2.228679
123.523125	1560.364526	5.272141	-0.023793	2.233840
123.967616	1568.401652	5.277146	-0.023881	2.238963
124.234096	1576.490784	5.282150	-0.023935	2.244090
124.366204	1584.572915	5.287155	-0.023965	2.249189
124.853926	1592.650116	5.292160	-0.024061	2.254305
125.110783	1600.734227	5.297165	-0.024114	2.259394
125.239295	1608.807085	5.302170	-0.024143	2.264452
125.580193	1616.905230	5.307174	-0.024211	2.269534
126.073517	1625.028545	5.312179	-0.024308	2.274633
126.138510	1633.099819	5.317184	-0.024325	2.279651
126.466630	1641.123111	5.322189	-0.024391	2.284651
126.770981	1649.182153	5.327194	-0.024453	2.289660
127.201722	1657.262693	5.332198	-0.024538	2.294682
127.162407	1665.333964	5.337203	-0.024536	2.299648
127.516411	1673.386997	5.342208	-0.024607	2.304625
127.988095	1681.441056	5.347213	-0.024699	2.309601
128.227779	1689.540229	5.352218	-0.024749	2.314575
128.690371	1697.579683	5.357222	-0.024840	2.319520
128.713451	1705.660935	5.362227	-0.024850	2.324444
129.100342	1713.732657	5.367232	-0.024927	2.329381
129.369374	1721.813080	5.372237	-0.024982	2.334304
129.611516	1729.870770	5.377242	-0.025032	2.339200
130.040290	1737.929508	5.382246	-0.025117	2.344101
130.038570	1746.030292	5.387251	-0.025121	2.348983
130.326834	1754.136508	5.392256	-0.025180	2.353881
130.599488	1762.181727	5.397261	-0.025236	2.358731
130.760913	1770.231568	5.402266	-0.025271	2.363565
131.108657	1778.286242	5.407270	-0.025341	2.368407
131.348307	1786.352010	5.412275	-0.025390	2.373237
131.691204	1794.436788	5.417280	-0.025459	2.378077
131.815283	1802.501857	5.422285	-0.025487	2.382877
132.179765	1810.550033	5.427290	-0.025560	2.387677
132.402060	1818.656385	5.432294	-0.025607	2.392491
132.354063	1826.738033	5.437299	-0.025603	2.397258
132.750827	1834.773265	5.442304	-0.025682	2.402024
133.031583	1842.823963	5.447309	-0.025739	2.406781
133.258625	1850.898987	5.452314	-0.025786	2.411538
133.523285	1858.978718	5.457318	-0.025840	2.416291
133.869688	1867.001164	5.462323	-0.025910	2.421008
134.353395	1875.042740	5.467328	-0.026005	2.425737
134.541221	1883.139707	5.472333	-0.026045	2.430466
134.922326	1891.262560	5.477338	-0.026121	2.435216
135.282555	1899.286833	5.482342	-0.026193	2.439898
135.598828	1907.283423	5.487347	-0.026257	2.444552
136.037605	1915.325068	5.492352	-0.026344	2.449231
136.420952	1923.402390	5.497357	-0.026420	2.453919
136.440370	1931.485806	5.502362	-0.026429	2.458573
136.738125	1939.533744	5.507366	-0.026489	2.463219
137.105766	1947.569967	5.512371	-0.026562	2.467855
137.493181	1955.648993	5.517376	-0.026640	2.472508
137.498590	1963.745096	5.522381	-0.026646	2.477133
137.752386	1971.770071	5.527386	-0.026698	2.481728
138.271409	1979.803934	5.532390	-0.026800	2.486338
138.445023	1987.874440	5.537395	-0.026837	2.490936
138.619486	1995.971989	5.542400	-0.026874	2.495540
138.825136	2004.024819	5.547405	-0.026918	2.500113
138.976122	2012.067227	5.552410	-0.026951	2.504667
139.188445	2020.167178	5.557414	-0.026995	2.509251
139.254913	2028.270032	5.562419	-0.027013	2.513816
139.595179	2036.301614	5.567424	-0.027081	2.518354
139.763019	2044.322656	5.572429	-0.027117	2.522864
140.068845	2052.355288	5.577434	-0.027179	2.527383
140.328857	2060.434352	5.582438	-0.027233	2.531917
140.450481	2068.489719	5.587443	-0.027260	2.536419
140.734691	2076.533987	5.592448	-0.027318	2.540918
141.099939	2084.557651	5.597453	-0.027391	2.545404
141.478159	2092.610386	5.602458	-0.027467	2.549899
141.811485	2100.690037	5.607462	-0.027534	2.554398
142.118541	2108.696770	5.612467	-0.027596	2.558846
142.363651	2116.759434	5.617472	-0.027647	2.563314
142.634196	2124.827156	5.622477	-0.027702	2.567778
142.982440	2132.854981	5.627482	-0.027772	2.572217
143.404006	2140.929778	5.632486	-0.027855	2.576680
143.615393	2148.986543	5.637491	-0.027900	2.581111
143.820994	2157.057443	5.642496	-0.027943	2.585541
144.000241	2165.135325	5.647501	-0.027981	2.589966
144.146272	2173.395466	5.652506	-0.028014	2.594480
144.600741	2181.351154	5.657510	-0.028103	2.598841
144.887822	2189.331303	5.662515	-0.028162	2.603197
145.335926	2197.338926	5.667520	-0.028250	2.607572
145.730324	2205.380220	5.672525	-0.028329	2.611954
145.820688	2213.440932	5.677530	-0.028350	2.616318
146.280706	2221.446774	5.682534	-0.028441	2.620670
146.539365	2229.485617	5.687539	-0.028494	2.625020
146.768140	2237.544841	5.692544	-0.028542	2.629371
147.026777	2245.635109	5.697549	-0.028595	2.633733
147.196541	2253.663948	5.702554	-0.028631	2.638049
147.536361	2261.699726	5.707558	-0.028700	2.642373
147.656479	2269.747495	5.712563	-0.028727	2.646682
148.030340	2277.795508	5.717568	-0.028802	2.651001
148.141230	2285.897269	5.722573	-0.028827	2.655324
148.328499	2293.910150	5.727578	-0.028867	2.659598
148.713952	2301.947166	5.732582	-0.028944	2.663890
149.037233	2309.973714	5.737587	-0.029009	2.668166
148.965246	2318.109218	5.742592	-0.029001	2.672467
149.104907	2326.175927	5.747597	-0.029032	2.676739
149.566006	2334.134921	5.752602	-0.029123	2.680967
149.935800	2342.177121	5.757606	-0.029197	2.685227
150.309610	2350.183707	5.762611	-0.029271	2.689461
150.463321	2358.296927	5.767616	-0.029305	2.693731
150.568999	2366.346056	5.772621	-0.029329	2.697957
150.905698	2374.367564	5.777626	-0.029397	2.702177
151.187833	2382.435864	5.782630	-0.029455	2.706411
151.315477	2390.492970	5.787635	-0.029483	2.710623
151.513701	2398.564439	5.792640	-0.029525	2.714840
151.886505	2406.573666	5.797645	-0.029600	2.719029
152.056977	2414.591321	5.802650	-0.029636	2.723204
152.308596	2422.658116	5.807654	-0.029688	2.727402
152.649812	2430.695463	5.812659	-0.029757	2.731584
152.905390	2438.765164	5.817664	-0.029809	2.735772
153.097723	2446.805845	5.822669	-0.029850	2.739934
153.325758	2454.825546	5.827674	-0.029898	2.744080
153.700959	2462.872317	5.832678	-0.029973	2.748244
154.027080	2470.963446	5.837683	-0.030038	2.752421
154.126393	2479.064521	5.842688	-0.030062	2.756583
154.370741	2487.064493	5.847693	-0.030112	2.760695
154.600616	2495.056247	5.852698	-0.030160	2.764797
154.969248	2503.108600	5.857702	-0.030234	2.768931
155.074055	2511.167289	5.862707	-0.030258	2.773047
155.372239	2519.212379	5.867712	-0.030319	2.777161
155.822922	2527.227838	5.872717	-0.030408	2.781263
155.774467	2535.286995	5.877722	-0.030404	2.785352
155.921888	2543.337073	5.882726	-0.030436	2.789441
156.195195	2551.382608	5.887731	-0.030492	2.793530
156.576717	2559.423856	5.892736	-0.030568	2.797617
156.639635	2567.481709	5.897741	-0.030585	2.801687
156.819891	2575.491912	5.902746	-0.030623	2.805734
157.071649	2583.549013	5.907750	-0.030675	2.809804
157.216032	2591.617851	5.912755	-0.030707	2.813867
157.518441	2599.649793	5.917760	-0.030768	2.817914
157.761581	2607.684038	5.922765	-0.030819	2.821954
158.072033	2615.712248	5.927770	-0.030881	2.825988
158.170030	2623.796378	5.932774	-0.030905	2.830033
158.246834	2631.868876	5.937779	-0.030924	2.834065
158.552464	2639.886118	5.942784	-0.030986	2.838076
158.798945	2647.909038	5.947789	-0.031037	2.842081
158.843505	2655.938646	5.952794	-0.031050	2.846073
159.245009	2663.951743	5.957798	-0.031130	2.850071
159.221262	2672.028793	5.962803	-0.031130	2.854070
159.366056	2680.073523	5.967808	-0.031162	2.858058
159.547163	2688.110308	5.972813	-0.031201	2.862038
159.701398	2696.125942	5.977818	-0.031235	2.866001
160.100798	2704.163930	5.982822	-0.031314	2.869983
160.272752	2712.226088	5.987827	-0.031351	2.873959
160.311957	2720.266026	5.992832	-0.031363	2.877910
160.580965	2728.290111	5.997837	-0.031418	2.881862
160.923558	2736.300581	6.002842	-0.031487	2.885805
161.216752	2744.349407	6.007846	-0.031547	2.889758
161.217659	2752.422062	6.012851	-0.031552	2.893702
161.431758	2760.478900	6.017856	-0.031597	2.897645
161.945118	2768.472676	6.022861	-0.031697	2.901567
162.006040	2776.532033	6.027866	-0.031714	2.905492
162.209960	2784.566626	6.032870	-0.031757	2.909407
162.513157	2792.676554	6.037875	-0.031818	2.913359
162.705661	2800.705389	6.042880	-0.031859	2.917260
162.861057	2808.737532	6.047885	-0.031893	2.921155
163.249926	2816.704501	6.052890	-0.031970	2.925026
163.505809	2824.754381	6.057894	-0.032023	2.928925
163.372333	2832.826505	6.062899	-0.032003	2.932808
163.564505	2840.871848	6.067904	-0.032044	2.936691
163.999366	2848.879467	6.072909	-0.032130	2.940563
164.117846	2856.878859	6.077914	-0.032157	2.944410
164.557306	2864.934801	6.082918	-0.032244	2.948295
164.475784	2873.013586	6.087923	-0.032234	2.952159
164.848185	2881.040854	6.092928	-0.032308	2.956017
165.042812	2889.069840	6.097933	-0.032349	2.959862
165.177216	2897.062798	6.102938	-0.032379	2.963681
165.617596	2905.102813	6.107942	-0.032466	2.967533
165.673506	2913.164509	6.112947	-0.032481	2.971371
165.936402	2921.224386	6.117952	-0.032535	2.975214
166.248260	2929.232320	6.122957	-0.032598	2.979029
166.347105	2937.257573	6.127962	-0.032622	2.982837
166.615638	2945.319973	6.132966	-0.032677	2.986666
166.858681	2953.351952	6.137971	-0.032727	2.990475
167.037660	2961.435509	6.142976	-0.032765	2.994299
167.360200	2969.438111	6.147981	-0.032830	2.998088
167.640827	2977.439514	6.152986	-0.032888	3.001870
167.983365	2985.484492	6.157990	-0.032956	3.005670
168.050770	2993.514243	6.162995	-0.032974	3.009444
168.175649	3001.571390	6.168000	-0.033002	3.013230
168.294614	3009.615355	6.173005	-0.033029	3.017004
168.506221	3017.647083	6.178010	-0.033074	3.020772
168.723765	3025.684993	6.183014	-0.033119	3.024539
169.042074	3033.713838	6.188019	-0.033184	3.028301
169.534258	3041.736091	6.193024	-0.033280	3.032065
169.763806	3049.825372	6.198029	-0.033328	3.035842
169.812556	3057.817957	6.203034	-0.033342	3.039560
169.967921	3065.866509	6.208038	-0.033376	3.043305
170.120067	3073.891719	6.213043	-0.033409	3.047035
170.209166	3081.946831	6.218048	-0.033431	3.050771
170.574397	3089.986838	6.223053	-0.033504	3.054508
170.576401	3098.000501	6.228058	-0.033509	3.058211
170.778268	3106.045363	6.233062	-0.033552	3.061934
170.977616	3114.046173	6.238067	-0.033594	3.065632
171.156515	3122.107689	6.243072	-0.033632	3.069352
171.356860	3130.220373	6.248077	-0.033674	3.073092
171.520473	3138.244088	6.253082	-0.033710	3.076785
171.937119	3146.231420	6.258086	-0.033792	3.080469
172.092182	3154.212766	6.263091	-0.033826	3.084133
172.317644	3162.241620	6.268096	-0.033873	3.087818
172.618671	3170.305362	6.273101	-0.033934	3.091518
172.666875	3178.338024	6.278106	-0.033948	3.095187
172.834353	3186.410045	6.283110	-0.033984	3.098876
172.933158	3194.412936	6.288115	-0.034008	3.102526
173.156626	3202.412822	6.293120	-0.034054	3.106175
173.499626	3210.475598	6.298125	-0.034123	3.109855
173.747768	3218.521776	6.303130	-0.034175	3.113518
173.929233	3226.542166	6.308134	-0.034213	3.117162
174.075028	3234.574204	6.313139	-0.034245	3.120805
174.215434	3242.585161	6.318144	-0.034277	3.124434
174.479995	3250.633329	6.323149	-0.034331	3.128082
174.627547	3258.676281	6.328154	-0.034363	3.131717
174.678639	3266.752033	6.333158	-0.034378	3.135359
174.710235	3274.757935	6.338163	-0.034389	3.138965
175.064585	3282.762905	6.343168	-0.034460	3.142579
175.260909	3290.796938	6.348173	-0.034501	3.146196
175.366487	3298.840840	6.353178	-0.034526	3.149809
175.608591	3306.909294	6.358182	-0.034576	3.153435
176.203684	3314.901126	6.363187	-0.034692	3.157038
176.217525	3322.927461	6.368192	-0.034699	3.160627
176.409425	3330.956847	6.373197	-0.034740	3.164221
176.511368	3338.939044	6.378202	-0.034764	3.167785
176.895258	3347.033451	6.383206	-0.034840	3.171408
177.011908	3355.080258	6.388211	-0.034867	3.174994
177.253832	3363.076384	6.393216	-0.034917	3.178559
177.673154	3371.107487	6.398221	-0.035000	3.182142
177.752020	3379.118515	6.403226	-0.035020	3.185699
178.146774	3387.159089	6.408230	-0.035098	3.189277
178.188035	3395.240528	6.413235	-0.035111	3.192855
178.310627	3403.299989	6.418240	-0.035139	3.196423
178.515183	3411.276535	6.423245	-0.035182	3.199953
178.521498	3419.297099	6.428250	-0.035188	3.203491
178.813627	3427.332090	6.433254	-0.035247	3.207043
178.893412	3435.364972	6.438259	-0.035267	3.210581
179.101959	3443.413806	6.443264	-0.035311	3.214127
179.250026	3451.470217	6.448269	-0.035344	3.217671
179.517067	3459.487380	6.453274	-0.035398	3.221198
179.865161	3467.483056	6.458278	-0.035468	3.224715
180.059005	3475.529903	6.463283	-0.035509	3.228245
180.235528	3483.585131	6.468288	-0.035547	3.231773
180.470947	3491.669523	6.473293	-0.035596	3.235313
180.562977	3499.635856	6.478298	-0.035618	3.238791
180.819317	3507.656502	6.483302	-0.035671	3.242297
180.924591	3515.671233	6.488307	-0.035695	3.245789
181.020835	3523.694770	6.493312	-0.035718	3.249281
181.383343	3531.730503	6.498317	-0.035791	3.252786
181.438472	3539.786795	6.503322	-0.035806	3.256283
181.806104	3547.795712	6.508326	-0.035879	3.259769
181.932888	3555.813795	6.513331	-0.035908	3.263245
182.040612	3563.866075	6.518336	-0.035933	3.266731
182.445836	3571.894102	6.523341	-0.036014	3.270215
182.723821	3579.920756	6.528346	-0.036070	3.273689
183.396455	3587.918072	6.533350	-0.036200	3.277163
183.392097	3595.952898	6.538355	-0.036205	3.280622
183.584252	3603.950848	6.543360	-0.036245	3.284070
183.917890	3611.982340	6.548365	-0.036313	3.287534
183.886103	3620.054638	6.553370	-0.036312	3.290997
184.170628	3628.109934	6.558374	-0.036370	3.294462
184.527553	3636.105376	6.563379	-0.036441	3.297900
184.789394	3644.122225	6.568384	-0.036495	3.301340
184.946651	3652.143015	6.573389	-0.036529	3.304775
185.112393	3660.183181	6.578394	-0.036565	3.308214
185.405211	3668.253465	6.583398	-0.036624	3.311667
185.436495	3676.299790	6.588403	-0.036635	3.315097
185.369919	3684.296344	6.593408	-0.036628	3.318498
185.798293	3692.316158	6.598413	-0.036713	3.321924
185.793980	3700.342125	6.603418	-0.036717	3.325333
186.118651	3708.349631	6.608422	-0.036782	3.328743
186.264956	3716.389254	6.613427	-0.036814	3.332156
186.479648	3724.445230	6.618432	-0.036859	3.335575
186.768141	3732.455882	6.623437	-0.036918	3.338974
186.951648	3740.465505	6.628442	-0.036957	3.342366
187.319879	3748.475444	6.633446	-0.037031	3.345761
187.275927	3756.557585	6.638451	-0.037028	3.349167
187.591905	3764.597526	6.643456	-0.037091	3.352566
188.044478	3772.642157	6.648461	-0.037181	3.355968
188.134581	3780.631292	6.653466	-0.037202	3.359330
188.439674	3788.663552	6.658470	-0.037264	3.362715
188.566758	3796.685817	6.663475	-0.037293	3.366085
188.859062	3804.678211	6.668480	-0.037352	3.369446
188.837289	3812.789824	6.673485	-0.037353	3.372842
188.968185	3820.808499	6.678490	-0.037383	3.376201
189.310889	3828.787337	6.683494	-0.037451	3.379547
189.407679	3836.816043	6.688499	-0.037474	3.382902
189.269201	3844.895136	6.693504	-0.037454	3.386267
189.682719	3852.881657	6.698509	-0.037536	3.389609
189.831652	3860.986333	6.703514	-0.037568	3.392988
189.943791	3869.049672	6.708518	-0.037594	3.396344
190.098810	3876.987373	6.713523	-0.037628	3.399647
190.381479	3884.966608	6.718528	-0.037686	3.402968
190.465001	3893.043465	6.723533	-0.037706	3.406320
190.679575	3901.005806	6.728538	-0.037751	3.409625
191.189897	3909.055604	6.733542	-0.037851	3.412973
191.426533	3917.110527	6.738547	-0.037900	3.416311
191.533711	3925.079007	6.743552	-0.037925	3.419605
191.933358	3933.128787	6.748557	-0.038004	3.422940
191.845535	3941.166824	6.753562	-0.037993	3.426250
191.899261	3949.208573	6.758566	-0.038008	3.429563
192.146380	3957.243823	6.763571	-0.038059	3.432877
192.468500	3965.258034	6.768576	-0.038124	3.436181
192.443570	3973.290884	6.773581	-0.038124	3.439478
192.660601	3981.269895	6.778586	-0.038170	3.442758
193.023606	3989.339307	6.783590	-0.038242	3.446077
193.177256	3997.342809	6.788595	-0.038276	3.449358
193.204789	4005.409243	6.793600	-0.038286	3.452658
193.402324	4013.490374	6.798605	-0.038328	3.455967
193.628365	4021.458456	6.803610	-0.038375	3.459227
193.974303	4029.486602	6.808614	-0.038444	3.462512
194.015270	4037.524671	6.813619	-0.038457	3.465788
194.357328	4045.538703	6.818624	-0.038526	3.469061
194.599314	4053.610670	6.823629	-0.038576	3.472352
194.612710	4061.625508	6.828634	-0.038583	3.475608
194.888091	4069.632536	6.833638	-0.038639	3.478867
194.950138	4077.632461	6.838643	-0.038656	3.482113
195.213850	4085.612444	6.843648	-0.038710	3.485354
195.671363	4093.678916	6.848653	-0.038800	3.488634
195.714905	4101.703743	6.853658	-0.038813	3.491880
195.865815	4109.737727	6.858662	-0.038846	3.495130
196.105308	4117.739857	6.863667	-0.038896	3.498367
196.280870	4125.759135	6.868672	-0.038934	3.501606
196.535165	4133.783696	6.873677	-0.038986	3.504847
196.452538	4141.811604	6.878682	-0.038975	3.508075
196.496778	4149.887577	6.883686	-0.038989	3.511324
196.723849	4157.909558	6.888691	-0.039036	3.514554
196.842873	4165.910748	6.893696	-0.039063	3.517769
197.021638	4173.961479	6.898701	-0.039101	3.521003
197.111910	4181.921208	6.903706	-0.039123	3.524194
197.328908	4189.976869	6.908710	-0.039169	3.527425
197.398821	4198.012146	6.913715	-0.039187	3.530641
198.019942	4206.034114	6.918720	-0.039307	3.533864
198.142042	4214.084211	6.923725	-0.039335	3.537081
198.200821	4222.082252	6.928730	-0.039351	3.540273
198.619366	4230.091839	6.933734	-0.039434	3.543476
198.741723	4238.162479	6.938739	-0.039462	3.546693
198.743947	4246.199233	6.943744	-0.039467	3.549889
199.011727	4254.312246	6.948749	-0.039522	3.553121
199.075069	4262.323679	6.953754	-0.039539	3.556303
199.321608	4270.262575	6.958758	-0.039589	3.559459
199.593605	4278.289508	6.963763	-0.039645	3.562648
199.870180	4286.284770	6.968768	-0.039702	3.565821
200.017547	4294.320491	6.973773	-0.039734	3.569004
199.877146	4302.372746	6.978778	-0.039713	3.572182
200.272698	4310.376234	6.983782	-0.039791	3.575354
200.454551	4318.386796	6.988787	-0.039830	3.578519
200.623584	4326.403889	6.993792	-0.039867	3.581684
200.910277	4334.412465	6.998797	-0.039925	3.584846
200.845417	4342.446589	7.003802	-0.039918	3.588005
200.974571	4350.491224	7.008806	-0.039947	3.591171
201.290387	4358.513659	7.013811	-0.040011	3.594331
201.627192	4366.516324	7.018816	-0.040079	3.597481
201.641939	4374.553240	7.023821	-0.040086	3.600632
201.960055	4382.521294	7.028826	-0.040150	3.603762
202.139555	4390.582925	7.033830	-0.040189	3.606922
202.252187	4398.587776	7.038835	-0.040215	3.610056
202.454352	4406.633261	7.043840	-0.040257	3.613205
202.583228	4414.735055	7.048845	-0.040286	3.616371
202.827193	4422.653300	7.053850	-0.040337	3.619465
203.048318	4430.738750	7.058854	-0.040383	3.622622
202.999553	4438.729154	7.063859	-0.040379	3.625732
203.419696	4446.753817	7.068864	-0.040462	3.628865
203.503461	4454.854885	7.073869	-0.040483	3.632015
203.665488	4462.856241	7.078874	-0.040518	3.635127
204.070738	4470.850878	7.083878	-0.040598	3.638239
204.208403	4478.892815	7.088883	-0.040629	3.641360
204.182143	4486.864323	7.093888	-0.040629	3.644447
204.563946	4494.929929	7.098893	-0.040705	3.647578
204.682480	4502.917304	7.103898	-0.040732	3.650670
204.731087	4511.018161	7.108902	-0.040746	3.653801
204.819970	4519.052849	7.113907	-0.040768	3.656904
204.787045	4527.027375	7.118912	-0.040767	3.659979
205.053759	4535.074196	7.123917	-0.040821	3.663086
205.216350	4543.060383	7.128922	-0.040856	3.666165
205.506012	4551.092697	7.133926	-0.040915	3.669263
205.701318	4559.133403	7.138931	-0.040957	3.672358
205.826644	4567.175105	7.143936	-0.040985	3.675449
205.963251	4575.186256	7.148941	-0.041015	3.678527
206.159582	4583.203461	7.153946	-0.041057	3.681605
206.356125	4591.175272	7.158950	-0.041099	3.684664
206.357109	4599.218170	7.163955	-0.041104	3.687742
206.629054	4607.218858	7.168960	-0.041159	3.690809
206.988936	4615.290015	7.173965	-0.041231	3.693902
207.112736	4623.314888	7.178970	-0.041259	3.696969
207.264006	4631.320941	7.183974	-0.041293	3.700026
207.583190	4639.324368	7.188979	-0.041357	3.703085
207.557900	4647.340578	7.193984	-0.041357	3.706137
207.699045	4655.391168	7.198989	-0.041388	3.709203
207.720028	4663.465303	7.203994	-0.041397	3.712273
207.991233	4671.534929	7.208998	-0.041453	3.715346
208.120432	4679.499531	7.214003	-0.041482	3.718372
208.349913	4687.476608	7.219008	-0.041530	3.721403
208.595383	4695.466691	7.224013	-0.041580	3.724436
208.771838	4703.499973	7.229018	-0.041618	3.727482
208.728586	4711.528277	7.234022	-0.041615	3.730518
209.064837	4719.599386	7.239027	-0.041683	3.733577
209.162541	4727.598890	7.244032	-0.041706	3.736601
209.227640	4735.613596	7.249037	-0.041723	3.739627
209.557654	4743.606608	7.254042	-0.041789	3.742649
209.804232	4751.620569	7.259046	-0.041840	3.745674
209.861177	4759.689456	7.264051	-0.041856	3.748713
210.006386	4767.697991	7.269056	-0.041888	3.751729
210.167164	4775.764427	7.274061	-0.041923	3.754764
210.332242	4783.732415	7.279066	-0.041958	3.757760
210.485473	4791.795796	7.284070	-0.041992	3.760790
210.826139	4799.784273	7.289075	-0.042060	3.763793
211.035709	4807.783975	7.294080	-0.042104	3.766795
211.066235	4815.863653	7.299085	-0.042115	3.769820
211.238380	4823.893635	7.304090	-0.042152	3.772827
211.596696	4831.917986	7.309094	-0.042224	3.775834
211.710389	4839.922696	7.314099	-0.042250	3.778826
211.739082	4847.927207	7.319104	-0.042260	3.781814
212.038324	4855.954494	7.324109	-0.042321	3.784813
212.218944	4863.984487	7.329114	-0.042360	3.787809
212.261038	4872.007369	7.334118	-0.042372	3.790796
212.428329	4880.095497	7.339123	-0.042409	3.793808
212.427979	4888.078216	7.344128	-0.042413	3.796775
212.604485	4896.063468	7.349133	-0.042451	3.799745
212.687124	4904.063099	7.354138	-0.042472	3.802715
213.168813	4912.059935	7.359142	-0.042566	3.805690
213.192482	4920.115319	7.364147	-0.042576	3.808675
213.304988	4928.137271	7.369152	-0.042602	3.811647
213.593331	4936.164614	7.374157	-0.042660	3.814623
213.862472	4944.169049	7.379162	-0.042715	3.817587
213.935626	4952.176761	7.384166	-0.042734	3.820546
214.083688	4960.216032	7.389171	-0.042767	3.823516
214.161518	4968.219914	7.394176	-0.042786	3.826469
214.209638	4976.250364	7.399181	-0.042800	3.829429
214.274183	4984.296298	7.404186	-0.042817	3.832393
214.648218	4992.302077	7.409190	-0.042892	3.835346
214.898715	5000.315230	7.414195	-0.042943	3.838297
215.063266	5008.321652	7.419200	-0.042979	3.841242
215.226447	5016.367556	7.424205	-0.043014	3.844198
215.353760	5024.365535	7.429210	-0.043043	3.847134
215.486715	5032.398346	7.434214	-0.043073	3.850081
215.698450	5040.456879	7.439219	-0.043117	3.853036
215.849426	5048.483238	7.444224	-0.043150	3.855976
216.135302	5056.500665	7.449229	-0.043208	3.858913
216.176810	5064.507843	7.454234	-0.043221	3.861839
216.452704	5072.503147	7.459238	-0.043277	3.864764
216.638622	5080.579748	7.464243	-0.043317	3.867714
216.516126	5088.576560	7.469248	-0.043299	3.870626
216.773010	5096.838320	7.474253	-0.043352	3.873640
217.107231	5104.808121	7.479258	-0.043419	3.876548
217.325603	5112.718151	7.484262	-0.043465	3.879429
217.147627	5120.749942	7.489267	-0.043437	3.882344
217.370483	5128.688886	7.494272	-0.043483	3.885231
217.644765	5136.721473	7.499277	-0.043539	3.888151
217.570715	5144.727874	7.504282	-0.043530	3.891053
217.853248	5152.772245	7.509286	-0.043588	3.893973
218.093301	5160.790513	7.514291	-0.043638	3.896880
218.086635	5168.769976	7.519296	-0.043641	3.899767
218.353864	5176.789425	7.524301	-0.043696	3.902671
218.542981	5184.801742	7.529306	-0.043736	3.905569
218.513257	5192.823659	7.534310	-0.043736	3.908464
218.742916	5200.877082	7.539315	-0.043784	3.911373
218.956547	5208.899303	7.544320	-0.043828	3.914268
219.007270	5216.930712	7.549325	-0.043843	3.917162
219.035267	5224.905899	7.554330	-0.043853	3.920032
219.387965	5232.914717	7.559334	-0.043924	3.922919
219.576724	5240.962237	7.564339	-0.043964	3.925814
219.739788	5248.940546	7.569344	-0.043999	3.928682
219.854859	5257.008119	7.574349	-0.044025	3.931579
219.957442	5265.028321	7.579354	-0.044050	3.934457
220.163819	5273.057110	7.584358	-0.044093	3.937337
220.261513	5281.066744	7.589363	-0.044116	3.940207
220.422800	5289.047691	7.594368	-0.044151	3.943065
220.822757	5297.087374	7.599373	-0.044231	3.945946
220.912544	5305.095898	7.604378	-0.044252	3.948809
221.117252	5313.156270	7.609382	-0.044295	3.951690
221.306025	5321.229524	7.614387	-0.044336	3.954573
221.210489	5329.221803	7.619392	-0.044323	3.957420
221.435906	5337.188501	7.624397	-0.044370	3.960262
221.523112	5345.204531	7.629402	-0.044391	3.963116
221.718419	5353.203639	7.634406	-0.044432	3.965965
221.898320	5361.229532	7.639411	-0.044471	3.968821
222.034360	5369.252824	7.644416	-0.044501	3.971673
222.273096	5377.310519	7.649421	-0.044550	3.974536
222.236430	5385.339578	7.654426	-0.044549	3.977383
222.604960	5393.290128	7.659430	-0.044622	3.980207
222.767378	5401.355782	7.664435	-0.044657	3.983066
222.924013	5409.344622	7.669440	-0.044692	3.985896
223.020272	5417.412664	7.674445	-0.044714	3.988751
223.283684	5425.437272	7.679450	-0.044768	3.991591
223.627904	5433.462226	7.684454	-0.044838	3.994430
223.591991	5441.534357	7.689459	-0.044836	3.997278
224.023438	5449.439462	7.694464	-0.044921	4.000073
224.172000	5457.519124	7.699469	-0.044954	4.002922
224.124512	5465.515032	7.704474	-0.044950	4.005737
224.351890	5473.509494	7.709478	-0.044997	4.008554
224.681348	5481.575270	7.714483	-0.045064	4.011395
224.620733	5489.631444	7.719488	-0.045057	4.014225
224.768894	5497.653760	7.724493	-0.045090	4.017044
224.905657	5505.650242	7.729498	-0.045120	4.019852
224.911155	5513.653711	7.734502	-0.045126	4.022658
225.301357	5521.669964	7.739507	-0.045204	4.025473
225.496490	5529.670193	7.744512	-0.045245	4.028277
225.555596	5537.757870	7.749517	-0.045261	4.031108
225.424317	5545.846108	7.754522	-0.045242	4.033934
225.582142	5553.872986	7.759526	-0.045276	4.036741
225.918408	5561.756544	7.764531	-0.045344	4.039499
226.111456	5569.757371	7.769536	-0.045385	4.042293
226.259863	5577.795277	7.774541	-0.045417	4.045098
226.528899	5585.814904	7.779546	-0.045472	4.047896
226.776413	5593.838414	7.784550	-0.045523	4.050694
226.991042	5601.886015	7.789555	-0.045568	4.053497
227.019192	5609.873414	7.794560	-0.045579	4.056275
227.311535	5617.895777	7.799565	-0.045638	4.059066
227.244396	5625.929662	7.804570	-0.045630	4.061855
227.446887	5633.904847	7.809574	-0.045673	4.064625
227.650694	5641.953060	7.814579	-0.045716	4.067418
227.733464	5649.964063	7.819584	-0.045736	4.070196
228.070252	5658.035212	7.824589	-0.045804	4.072995
228.057972	5666.046731	7.829594	-0.045807	4.075767
228.187135	5674.006542	7.834598	-0.045836	4.078521
228.514917	5682.046096	7.839603	-0.045902	4.081304
228.346133	5690.018790	7.844608	-0.045875	4.084055
228.820862	5698.088061	7.849613	-0.045969	4.086846
228.879141	5706.075314	7.854618	-0.045985	4.089601
229.049741	5714.119768	7.859622	-0.046021	4.092375
229.126570	5722.181579	7.864627	-0.046041	4.095153
229.523838	5730.143899	7.869632	-0.046120	4.097898
229.589626	5738.186285	7.874637	-0.046137	4.100665
229.640441	5746.172918	7.879642	-0.046151	4.103411
229.908923	5754.208438	7.884646	-0.046206	4.106174
230.153569	5762.250396	7.889651	-0.046257	4.108937
230.221369	5770.264503	7.894656	-0.046274	4.111687
230.529779	5778.336912	7.899661	-0.046337	4.114457
230.542799	5786.291014	7.904666	-0.046344	4.117182
230.844345	5794.258808	7.909670	-0.046405	4.119913
230.984123	5802.359446	7.914675	-0.046436	4.122686
231.209568	5810.303473	7.919680	-0.046483	4.125404
231.265295	5818.376085	7.924685	-0.046499	4.128162
231.378012	5826.378860	7.929690	-0.046525	4.130896
231.656401	5834.435904	7.934694	-0.046581	4.133648
231.641391	5842.516358	7.939699	-0.046584	4.136402
231.466725	5850.463094	7.944704	-0.046556	4.139107
231.788887	5858.506382	7.949709	-0.046621	4.141850
231.956794	5866.459650	7.954714	-0.046657	4.144558
232.099274	5874.521964	7.959718	-0.046689	4.147301
232.365119	5882.555020	7.964723	-0.046743	4.150034
232.616255	5890.576525	7.969728	-0.046795	4.152760
233.013277	5898.631479	7.974733	-0.046874	4.155498
233.090083	5906.617327	7.979738	-0.046893	4.158207
233.170028	5914.597253	7.984742	-0.046913	4.160912
233.343440	5922.631784	7.989747	-0.046950	4.163636
233.188482	5930.651428	7.994752	-0.046926	4.166348
233.451462	5938.664902	7.999757	-0.046980	4.169061
233.732820	5946.704347	8.004762	-0.047038	4.171782
233.702156	5954.721665	8.009766	-0.047037	4.174489
233.871219	5962.748660	8.014771	-0.047074	4.177201
233.991194	5970.728871	8.019776	-0.047101	4.179894
234.299463	5978.744240	8.024781	-0.047163	4.182600
234.189399	5986.729435	8.029786	-0.047148	4.185289
234.409754	5994.802710	8.034790	-0.047194	4.188009
234.886587	6002.832233	8.039795	-0.047287	4.190716
234.756406	6010.898651	8.044800	-0.047268	4.193427
235.201840	6018.999334	8.049805	-0.047356	4.196154
235.229448	6026.849910	8.054810	-0.047366	4.198790
235.411285	6034.902533	8.059814	-0.047405	4.201494
235.589365	6042.883252	8.064819	-0.047443	4.204173
235.603523	6050.871431	8.069824	-0.047451	4.206850
235.825861	6058.902115	8.074829	-0.047497	4.209542
235.864292	6066.961400	8.079834	-0.047509	4.212240
235.978946	6074.972206	8.084838	-0.047536	4.214921
236.181227	6083.007002	8.089843	-0.047578	4.217609
236.276515	6090.929640	8.094848	-0.047601	4.220257
236.579026	6098.996096	8.099853	-0.047662	4.222953
236.922058	6106.989883	8.104858	-0.047731	4.225624
237.141213	6115.016878	8.109862	-0.047777	4.228302
237.284143	6123.062537	8.114867	-0.047809	4.230985
237.418332	6131.076109	8.119872	-0.047838	4.233655
237.549161	6139.121174	8.124877	-0.047868	4.236334
237.563553	6147.102431	8.129882	-0.047875	4.238988
237.669240	6155.107712	8.134886	-0.047900	4.241650
237.896426	6163.108050	8.139891	-0.047947	4.244310
238.102508	6171.172427	8.144896	-0.047991	4.246989
238.402324	6179.155589	8.149901	-0.048052	4.249640
238.638301	6187.196500	8.154906	-0.048100	4.252308
238.827657	6195.211801	8.159910	-0.048141	4.254965
238.902083	6203.316449	8.164915	-0.048160	4.257650
239.048578	6211.227051	8.169920	-0.048192	4.260269
239.264299	6219.299369	8.174925	-0.048237	4.262940
239.232992	6227.275731	8.179930	-0.048236	4.265576
239.356435	6235.342735	8.184934	-0.048264	4.268242
239.585103	6243.376114	8.189939	-0.048312	4.270895
239.528899	6251.437190	8.194944	-0.048306	4.273554
239.707997	6259.479161	8.199949	-0.048345	4.276207
239.755299	6267.421544	8.204954	-0.048358	4.278824
240.001371	6275.430123	8.209958	-0.048409	4.281463
240.059175	6283.440937	8.214963	-0.048425	4.284100
240.105172	6291.494049	8.219968	-0.048438	4.286748
240.339228	6299.455295	8.224973	-0.048487	4.289367
240.356388	6307.536230	8.229978	-0.048495	4.292021
240.615881	6315.535349	8.234982	-0.048548	4.294649
240.752787	6323.588167	8.239987	-0.048579	4.297292
240.890916	6331.508804	8.244992	-0.048610	4.299889
241.081780	6339.579813	8.249997	-0.048650	4.302535
240.948592	6347.554869	8.255002	-0.048630	4.305146
241.217203	6355.591069	8.260006	-0.048685	4.307777
241.304383	6363.651832	8.265011	-0.048706	4.310414
241.398159	6371.669645	8.270016	-0.048729	4.313036
241.718004	6379.648924	8.275021	-0.048793	4.315644
241.938627	6387.667963	8.280026	-0.048839	4.318264
242.133072	6395.659055	8.285030	-0.048881	4.320872
242.503816	6403.669299	8.290035	-0.048955	4.323486
242.508695	6411.681196	8.295040	-0.048961	4.326097
242.595135	6419.699018	8.300045	-0.048982	4.328709
242.709339	6427.771014	8.305050	-0.049008	4.331336
242.916085	6435.772986	8.310054	-0.049051	4.333940
243.004247	6443.822760	8.315059	-0.049073	4.336558
243.168556	6451.808525	8.320064	-0.049108	4.339153
243.374288	6459.853099	8.325069	-0.049152	4.341766
243.486928	6467.788092	8.330074	-0.049178	4.344341
243.463443	6475.842383	8.335078	-0.049178	4.346953
243.880078	6483.870319	8.340083	-0.049261	4.349557
243.788118	6491.892365	8.345088	-0.049249	4.352155
244.033205	6499.995364	8.350093	-0.049299	4.354779
244.264407	6508.023505	8.355098	-0.049347	4.357378
244.576200	6515.938062	8.360102	-0.049410	4.359938
244.733300	6523.947417	8.365107	-0.049444	4.362527
244.778257	6531.938623	8.370112	-0.049458	4.365108
244.989187	6539.987532	8.375117	-0.049502	4.367706
245.283796	6547.991325	8.380122	-0.049562	4.370290
245.277917	6556.045342	8.385126	-0.049566	4.372886
245.604230	6564.085376	8.390131	-0.049632	4.375477
245.600954	6572.069441	8.395136	-0.049636	4.378048
245.619502	6580.060717	8.400141	-0.049644	4.380619
245.631019	6588.054888	8.405146	-0.049651	4.383190
245.747150	6596.070365	8.410150	-0.049678	4.385766
245.805185	6604.119829	8.415155	-0.049694	4.388352
245.884566	6612.126027	8.420160	-0.049714	4.390922
246.060616	6620.147946	8.425165	-0.049751	4.393497
246.325707	6628.186769	8.430170	-0.049806	4.396075
246.527654	6636.152542	8.435174	-0.049848	4.398629
246.738617	6644.244782	8.440179	-0.049893	4.401221
246.719080	6652.151493	8.445184	-0.049894	4.403752
246.746999	6660.220148	8.450189	-0.049904	4.406333
246.768319	6668.242857	8.455194	-0.049913	4.408898
247.111722	6676.265148	8.460198	-0.049982	4.411462
247.326598	6684.324584	8.465203	-0.050027	4.414037
247.222097	6692.336995	8.470208	-0.050012	4.416593
247.850385	6700.313450	8.475213	-0.050134	4.419140
247.887832	6708.391849	8.480218	-0.050146	4.421715
247.677112	6716.332599	8.485222	-0.050112	4.424243
247.970255	6724.433248	8.490227	-0.050172	4.426824
248.176121	6732.372177	8.495232	-0.050215	4.429351
248.306946	6740.448396	8.500237	-0.050244	4.431920
248.342991	6748.508097	8.505242	-0.050256	4.434481
248.786370	6756.514706	8.510246	-0.050344	4.437026
248.857852	6764.494793	8.515251	-0.050362	4.439560
248.852901	6772.530709	8.520256	-0.050366	4.442109
249.216724	6780.482617	8.525261	-0.050439	4.444632
249.300522	6788.559156	8.530266	-0.050459	4.447192
249.383523	6796.496436	8.535270	-0.050480	4.449706
249.530959	6804.572589	8.540275	-0.050512	4.452263
249.656025	6812.602398	8.545280	-0.050540	4.454803
249.760702	6820.656855	8.550285	-0.050565	4.457350
249.911730	6828.604712	8.555290	-0.050598	4.459862
250.100628	6836.615997	8.560295	-0.050638	4.462393
250.423069	6844.609562	8.565299	-0.050703	4.464917
250.492457	6852.679023	8.570304	-0.050721	4.467463
250.720183	6860.667122	8.575309	-0.050768	4.469982
250.827118	6868.712714	8.580314	-0.050793	4.472517
251.005535	6876.724451	8.585319	-0.050831	4.475041
251.178657	6884.774582	8.590323	-0.050869	4.477575
251.516512	6892.690593	8.595328	-0.050936	4.480066
251.524129	6900.758626	8.600333	-0.050943	4.482602
251.612880	6908.774748	8.605338	-0.050964	4.485121
251.697640	6916.778553	8.610343	-0.050985	4.487635
251.929190	6924.827238	8.615347	-0.051033	4.490161
251.886387	6932.824451	8.620352	-0.051030	4.492670
251.956491	6940.868892	8.625357	-0.051048	4.495192
252.290710	6948.880561	8.630362	-0.051116	4.497703
252.287785	6956.854016	8.635367	-0.051120	4.500199
252.525973	6964.914593	8.640371	-0.051169	4.502722
252.758263	6972.864023	8.645376	-0.051217	4.505209
252.850405	6980.892055	8.650381	-0.051240	4.507719
252.746546	6988.953213	8.655386	-0.051225	4.510237
252.876241	6996.992956	8.660391	-0.051254	4.512748
253.133204	7005.041237	8.665395	-0.051307	4.515260
253.060521	7012.997515	8.670400	-0.051299	4.517742
253.265489	7020.961077	8.675405	-0.051342	4.520225
253.526780	7028.992845	8.680410	-0.051395	4.522728
253.559210	7036.977642	8.685415	-0.051406	4.525214
253.901055	7045.025927	8.690419	-0.051475	4.527719
253.864121	7053.008056	8.695424	-0.051473	4.530202
254.030757	7061.062548	8.700429	-0.051509	4.532706
254.179305	7069.097558	8.705434	-0.051542	4.535203
254.336962	7077.097783	8.710439	-0.051576	4.537687
254.496530	7085.105468	8.715443	-0.051611	4.540173
254.468956	7093.100561	8.720448	-0.051611	4.542653
254.605701	7101.102132	8.725453	-0.051641	4.545133
255.084209	7109.154690	8.730458	-0.051735	4.547629
254.989522	7117.125061	8.735463	-0.051722	4.550097
255.157426	7125.221532	8.740467	-0.051759	4.552603
255.458308	7133.244166	8.745472	-0.051820	4.555085
255.746079	7141.285503	8.750477	-0.051878	4.557571
255.726436	7149.237687	8.755482	-0.051880	4.560028
255.648977	7157.256086	8.760487	-0.051870	4.562504
255.919012	7165.267319	8.765491	-0.051925	4.564977
255.877425	7173.291273	8.770496	-0.051923	4.567453
256.127808	7181.265852	8.775501	-0.051974	4.569911
256.255586	7189.344566	8.780506	-0.052003	4.572401
256.138015	7197.326110	8.785511	-0.051986	4.574859
256.490014	7205.430215	8.790515	-0.052057	4.577354
256.613783	7213.351731	8.795520	-0.052085	4.579791
256.898587	7221.439606	8.800525	-0.052143	4.582278
256.911046	7229.389366	8.805530	-0.052150	4.584721
257.047278	7237.432578	8.810535	-0.052180	4.587191
257.406135	7245.463457	8.815539	-0.052252	4.589657
257.522077	7253.488052	8.820544	-0.052279	4.592119
257.661354	7261.537335	8.825549	-0.052310	4.594587
257.939928	7269.593865	8.830554	-0.052367	4.597056
258.056250	7277.479686	8.835559	-0.052393	4.599471
258.187919	7285.576762	8.840563	-0.052423	4.601950
258.167948	7293.480393	8.845568	-0.052424	4.604369
258.457056	7301.573823	8.850573	-0.052483	4.606844
258.543594	7309.563520	8.855578	-0.052504	4.609286
258.673412	7317.598373	8.860583	-0.052533	4.611740
258.808183	7325.609948	8.865587	-0.052563	4.614186
258.887883	7333.629922	8.870592	-0.052583	4.616634
258.973515	7341.638832	8.875597	-0.052604	4.619076
259.273014	7349.690035	8.880602	-0.052664	4.621531
259.436123	7357.614346	8.885607	-0.052700	4.623945
259.547031	7365.715113	8.890611	-0.052725	4.626412
259.699250	7373.681777	8.895616	-0.052759	4.628836
259.981539	7381.769887	8.900621	-0.052816	4.631296
260.059513	7389.803564	8.905626	-0.052836	4.633739
260.388167	7397.788494	8.910631	-0.052902	4.636165
260.472346	7405.771115	8.915635	-0.052923	4.638589
260.444147	7413.757720	8.920640	-0.052922	4.641013
260.537463	7421.757006	8.925645	-0.052945	4.643440
260.849044	7429.821819	8.930650	-0.053008	4.645885
260.769088	7437.812691	8.935655	-0.052998	4.648307
261.060935	7445.864434	8.940659	-0.053057	4.650745
261.189899	7453.873612	8.945664	-0.053086	4.653170
261.423691	7461.902843	8.950669	-0.053135	4.655599
261.478688	7469.899612	8.955674	-0.053150	4.658017
261.561747	7477.865540	8.960679	-0.053170	4.660425
261.881159	7485.953335	8.965683	-0.053235	4.662868
261.746802	7493.895788	8.970688	-0.053215	4.665266
261.950217	7501.958562	8.975693	-0.053258	4.667699
262.185958	7509.969864	8.980698	-0.053306	4.670116
262.311625	7518.037737	8.985703	-0.053335	4.672548
262.330290	7526.122831	8.990707	-0.053343	4.674984
262.422119	7534.045573	8.995712	-0.053365	4.677370
262.714312	7542.028424	9.000717	-0.053425	4.679772
263.057892	7550.060409	9.005722	-0.053494	4.682188
262.893583	7558.004541	9.010727	-0.053468	4.684577
263.336040	7566.109951	9.015731	-0.053555	4.687012
263.323271	7574.014315	9.020736	-0.053558	4.689386
263.323352	7582.087113	9.025741	-0.053563	4.691810
263.399972	7590.118787	9.030746	-0.053582	4.694220
263.632225	7598.198334	9.035751	-0.053630	4.696642
263.840153	7606.124675	9.040755	-0.053674	4.699018
263.947355	7614.146141	9.045760	-0.053699	4.701421
263.966197	7622.173216	9.050765	-0.053708	4.703824
264.223269	7630.190504	9.055770	-0.053760	4.706223
264.099793	7638.152758	9.060775	-0.053742	4.708605
264.468253	7646.261708	9.065779	-0.053816	4.711029
264.522026	7654.256502	9.070784	-0.053831	4.713418
264.571029	7662.236521	9.075789	-0.053845	4.715801
264.789036	7670.292092	9.080794	-0.053891	4.718206
265.057752	7678.216232	9.085799	-0.053946	4.720569
265.181382	7686.297126	9.090803	-0.053974	4.722979
265.206517	7694.322658	9.095808	-0.053983	4.725371
265.461193	7702.328149	9.100813	-0.054036	4.727755
265.574803	7710.367943	9.105818	-0.054062	4.730149
265.631838	7718.418671	9.110823	-0.054077	4.732545
265.695543	7726.427380	9.115827	-0.054094	4.734927
265.732585	7734.449344	9.120832	-0.054106	4.737312
265.860704	7742.415335	9.125837	-0.054135	4.739678
265.972440	7750.451436	9.130842	-0.054161	4.742065
266.163876	7758.404103	9.135847	-0.054201	4.744425
266.660820	7766.473514	9.140851	-0.054299	4.746818
266.663026	7774.440753	9.145856	-0.054304	4.749181
266.813609	7782.530545	9.150861	-0.054337	4.751578
266.934412	7790.573559	9.155866	-0.054365	4.753960
267.108419	7798.565373	9.160871	-0.054402	4.756326
267.374829	7806.557037	9.165875	-0.054457	4.758691
267.582507	7814.539423	9.170880	-0.054500	4.761051
267.680623	7822.537219	9.175885	-0.054524	4.763415
267.678766	7830.580085	9.180890	-0.054528	4.765792
267.838424	7838.584566	9.185895	-0.054563	4.768156
268.072821	7846.613068	9.190899	-0.054612	4.770525
267.921058	7854.655544	9.195904	-0.054588	4.772899
268.144261	7862.626361	9.200909	-0.054635	4.775249
268.508188	7870.705809	9.205914	-0.054708	4.777629
268.427752	7878.683867	9.210919	-0.054698	4.779980
268.520112	7886.709528	9.215923	-0.054720	4.782343
268.741255	7894.662459	9.220928	-0.054766	4.784683
268.959134	7902.702125	9.225933	-0.054811	4.787047
269.182912	7910.733196	9.230938	-0.054858	4.789408
269.167521	7918.683080	9.235943	-0.054860	4.791744
269.398477	7926.826460	9.240947	-0.054908	4.794135
269.520158	7934.812852	9.245952	-0.054936	4.796480
269.332223	7942.778372	9.250957	-0.054906	4.798818
269.822065	7950.833539	9.255962	-0.055002	4.801178
269.877763	7958.787161	9.260967	-0.055017	4.803510
269.986090	7966.831813	9.265971	-0.055042	4.805867
270.160942	7974.836725	9.270976	-0.055080	4.808210
270.307891	7982.819572	9.275981	-0.055112	4.810547
270.393085	7990.280279	9.280986	-0.055133	4.812729
270.228314	7994.823596	9.285991	-0.055105	4.814059

270.506816	7997.331647	9.290995	-0.055158	4.814791
270.636472	7998.616093	9.296000	-0.055183	4.815166
270.743484	7998.966983	9.301005	-0.055203	4.815268
270.891087	8000.086338	9.306010	-0.055231	4.815595
270.871552	8000.058233	9.311015	-0.055227	4.815587
270.773375	8000.058747	9.316019	-0.055208	4.815587
270.891377	8000.046766	9.321024	-0.055230	4.815583
271.076197	8000.083930	9.326029	-0.055264	4.815593
270.906491	8000.086481	9.331034	-0.055232	4.815595
271.024572	8000.037126	9.336039	-0.055254	4.815580
271.388791	8000.076147	9.341043	-0.055322	4.815589
271.215020	8000.042323	9.346048	-0.055289	4.815580
271.477862	8000.056198	9.351053	-0.055338	4.815583
271.522228	8000.064375	9.356058	-0.055346	4.815585
271.388693	8000.024800	9.361063	-0.055321	4.815574
271.608054	8000.028355	9.366067	-0.055361	4.815574
271.587296	8000.027995	9.371072	-0.055357	4.815574
271.707409	8000.071580	9.376077	-0.055379	4.815587
271.889175	8000.068115	9.381082	-0.055413	4.815585
271.604285	8000.045293	9.386087	-0.055359	4.815579
271.763289	8000.077766	9.391091	-0.055389	4.815588
271.681099	8000.016601	9.396096	-0.055373	4.815571
271.746835	8000.042213	9.401101	-0.055385	4.815578
271.950359	8000.042307	9.406106	-0.055423	4.815577
271.968469	8000.052192	9.411111	-0.055426	4.815580
272.111494	8000.061978	9.416115	-0.055452	4.815582
272.035351	8000.054308	9.421120	-0.055438	4.815580
271.981656	8000.077972	9.426125	-0.055428	4.815587
272.030510	8000.039235	9.431130	-0.055437	4.815576
271.911001	8000.063962	9.436135	-0.055414	4.815583
272.093523	8000.098954	9.441139	-0.055448	4.815593
271.802764	8000.031184	9.446144	-0.055393	4.815574
271.850994	8000.058647	9.451149	-0.055402	4.815582
272.113494	8000.079993	9.456154	-0.055451	4.815587
271.957886	8000.044328	9.461159	-0.055422	4.815577
271.960053	8000.080651	9.466163	-0.055422	4.815588
271.861625	8000.033104	9.471168	-0.055403	4.815575
272.089119	8000.048539	9.476173	-0.055445	4.815578
272.026738	8000.046432	9.481178	-0.055433	4.815578
271.888737	8000.032413	9.486183	-0.055408	4.815574
272.028760	8000.068848	9.491187	-0.055433	4.815584
271.941364	8000.035364	9.496192	-0.055417	4.815575
272.257033	8000.053306	9.501197	-0.055475	4.815579
272.261566	8000.065105	9.506202	-0.055476	4.815582
272.359075	8000.047451	9.511207	-0.055494	4.815577
272.147551	8000.051455	9.516211	-0.055454	4.815579
272.098960	8000.038894	9.521216	-0.055445	4.815575
272.026134	8000.049432	9.526221	-0.055431	4.815579
272.199434	8000.054372	9.531226	-0.055463	4.815579
272.190491	8000.031778	9.536231	-0.055461	4.815573
272.291420	8000.084663	9.541235	-0.055480	4.815588
272.325241	8000.044612	9.546240	-0.055486	4.815576
272.360787	8000.057985	9.551245	-0.055492	4.815580
272.421950	8000.080320	9.556250	-0.055503	4.815586
272.385043	8000.045523	9.561255	-0.055496	4.815576
272.307213	8000.063454	9.566259	-0.055481	4.815582
272.378200	8000.048572	9.571264	-0.055494	4.815577
272.447267	8000.065695	9.576269	-0.055507	4.815582
272.371020	8000.065498	9.581274	-0.055493	4.815582
272.256316	8000.064673	9.586279	-0.055471	4.815582
272.397888	8000.085116	9.591283	-0.055497	4.815587
272.463706	8000.094711	9.596288	-0.055509	4.815590
272.365188	8000.110169	9.601293	-0.055491	4.815595
272.423608	8000.182652	9.606298	-0.055501	4.815616
272.463761	8000.085036	9.611303	-0.055508	4.815587
272.385549	8000.092282	9.616307	-0.055494	4.815590
272.390875	8000.064581	9.621312	-0.055494	4.815582
272.521531	8000.052808	9.626317	-0.055518	4.815577
272.627063	8000.063051	9.631322	-0.055538	4.815580
272.434345	8000.038527	9.636327	-0.055502	4.815574
272.632810	8000.084460	9.641331	-0.055538	4.815586
272.545212	8000.048836	9.646336	-0.055522	4.815576
272.514701	8000.057928	9.651341	-0.055516	4.815579
272.602259	8000.076421	9.656346	-0.055532	4.815584
272.664997	8000.052861	9.661351	-0.055543	4.815577
272.817426	8000.077752	9.666355	-0.055572	4.815583
272.818276	8000.063861	9.671360	-0.055571	4.815579
272.636224	8000.075821	9.676365	-0.055537	4.815584
272.619324	8000.103290	9.681370	-0.055534	4.815592
272.693832	8000.047883	9.686375	-0.055548	4.815575
272.801727	8000.109426	9.691379	-0.055567	4.815593
272.711861	8000.137840	9.696384	-0.055550	4.815601
272.528701	8000.092113	9.701389	-0.055516	4.815589
272.640480	8000.106731	9.706394	-0.055537	4.815593
272.674356	8000.073088	9.711399	-0.055543	4.815583
272.929578	8000.115676	9.716403	-0.055590	4.815594
272.526975	8000.086659	9.721408	-0.055515	4.815587
272.569249	8000.071308	9.726413	-0.055522	4.815583
272.833741	8000.092688	9.731418	-0.055571	4.815588
272.663679	8000.054651	9.736423	-0.055539	4.815577
272.855841	8000.089802	9.741427	-0.055575	4.815587
272.879329	8000.112590	9.746432	-0.055579	4.815593
272.798910	8000.084558	9.751437	-0.055564	4.815586
272.868302	8000.083533	9.756442	-0.055577	4.815585
272.979198	8000.073573	9.761447	-0.055597	4.815582
272.983042	8000.117400	9.766451	-0.055597	4.815594
272.869704	8000.100578	9.771456	-0.055576	4.815590
272.970974	8000.071238	9.776461	-0.055595	4.815581
273.013088	8000.109281	9.781466	-0.055602	4.815592
272.926946	8000.054458	9.786471	-0.055586	4.815576
272.988146	8000.088540	9.791475	-0.055597	4.815586
273.137360	8000.081342	9.796480	-0.055625	4.815583
272.871231	8000.065231	9.801485	-0.055575	4.815580
272.950964	8000.081461	9.806490	-0.055590	4.815584
272.902871	8000.046481	9.811495	-0.055580	4.815574
272.865500	8000.091771	9.816499	-0.055573	4.815587
272.849064	8000.046628	9.821504	-0.055570	4.815574
272.887930	8000.054716	9.826509	-0.055577	4.815577
272.980555	8000.092515	9.831514	-0.055594	4.815587
272.827491	8000.070774	9.836519	-0.055565	4.815582
272.845126	8000.096670	9.841523	-0.055568	4.815589
273.048995	8000.110654	9.846528	-0.055606	4.815592
272.870108	8000.093831	9.851533	-0.055572	4.815588
273.044157	8000.094513	9.856538	-0.055604	4.815587
273.013829	8000.051279	9.861543	-0.055598	4.815575
273.242974	8000.111597	9.866547	-0.055641	4.815592
273.051367	8000.068935	9.871552	-0.055605	4.815580
272.934717	8000.085165	9.876557	-0.055583	4.815585
273.221326	8000.097296	9.881562	-0.055636	4.815587
273.045018	8000.062359	9.886567	-0.055603	4.815578
273.084127	8000.068315	9.891571	-0.055610	4.815580
272.958581	8000.043819	9.896576	-0.055586	4.815573
273.013199	8000.064979	9.901581	-0.055596	4.815579
273.031896	8000.086621	9.906586	-0.055600	4.815585
273.210518	8000.068155	9.911591	-0.055633	4.815579
273.372064	8000.085721	9.916595	-0.055663	4.815583
273.241788	8000.102796	9.921600	-0.055638	4.815589
273.245381	8000.076134	9.926605	-0.055638	4.815581
273.243275	8000.150835	9.931610	-0.055638	4.815603
273.130349	8000.091301	9.936615	-0.055617	4.815586
273.110997	8000.093100	9.941619	-0.055613	4.815587
273.244179	8000.085640	9.946624	-0.055637	4.815584
273.169537	8000.075857	9.951629	-0.055623	4.815582
273.003027	8000.100885	9.956634	-0.055592	4.815590
272.964897	8000.056456	9.961639	-0.055584	4.815577
273.246072	8000.109079	9.966643	-0.055637	4.815591
273.246956	8000.078101	9.971648	-0.055636	4.815582
273.001410	8000.064462	9.976653	-0.055591	4.815579
273.243563	8000.075867	9.981658	-0.055635	4.815581
273.284617	8000.049817	9.986663	-0.055643	4.815573
273.288739	8000.096852	9.991667	-0.055643	4.815587
273.404563	8000.063478	9.996672	-0.055665	4.815577
273.256046	8000.074916	10.001677	-0.055637	4.815581
273.350704	8000.093526	10.006682	-0.055654	4.815586
273.364173	8000.052074	10.011687	-0.055656	4.815574
273.501996	8000.073525	10.016691	-0.055682	4.815579
273.248531	8000.061892	10.021696	-0.055634	4.815577
273.280757	8000.065600	10.026701	-0.055640	4.815578
273.299302	8000.078696	10.031706	-0.055643	4.815582
273.263248	8000.047116	10.036711	-0.055636	4.815573
273.234578	8000.084004	10.041715	-0.055631	4.815584
273.541187	8000.100733	10.046720	-0.055688	4.815587
273.543983	8000.107165	10.051725	-0.055688	4.815589
273.537655	8000.093157	10.056730	-0.055686	4.815585
273.485457	8000.070924	10.061735	-0.055676	4.815579
273.625529	8000.093480	10.066739	-0.055702	4.815585
273.468625	8000.105849	10.071744	-0.055673	4.815589
273.406955	8000.087734	10.076749	-0.055661	4.815584
273.510407	8000.093672	10.081754	-0.055680	4.815585
273.370030	8000.047574	10.086759	-0.055654	4.815572
273.301141	8000.100893	10.091763	-0.055641	4.815588
273.246375	8000.071144	10.096768	-0.055630	4.815580
273.283852	8000.079209	10.101773	-0.055637	4.815582
273.439473	8000.097746	10.106778	-0.055666	4.815587
273.388192	8000.053102	10.111783	-0.055656	4.815574
273.412009	8000.101526	10.116787	-0.055660	4.815588
273.614930	8000.094137	10.121792	-0.055698	4.815585
273.546449	8000.068435	10.126797	-0.055685	4.815578
273.482971	8000.139998	10.131802	-0.055673	4.815599
273.468227	8000.083134	10.136807	-0.055670	4.815582
273.622841	8000.134761	10.141811	-0.055698	4.815597
273.443528	8000.112590	10.146816	-0.055664	4.815591
273.443087	8000.130717	10.151821	-0.055664	4.815596
273.445944	8000.127538	10.156826	-0.055664	4.815596
273.250097	8000.083738	10.161831	-0.055628	4.815584
273.411369	8000.111979	10.166835	-0.055657	4.815591
273.681796	8000.091808	10.171840	-0.055708	4.815584
273.555659	8000.101475	10.176845	-0.055684	4.815587
273.602844	8000.127854	10.181850	-0.055692	4.815595
273.620729	8000.089678	10.186855	-0.055695	4.815584
273.773012	8000.133792	10.191859	-0.055724	4.815596
273.421571	8000.098132	10.196864	-0.055658	4.815587
273.515705	8000.101783	10.201869	-0.055675	4.815588
273.430884	8000.178337	10.206874	-0.055659	4.815611
273.268135	8000.087020	10.211879	-0.055629	4.815585
273.479799	8000.119287	10.216883	-0.055668	4.815593
273.541732	8000.108529	10.221888	-0.055679	4.815590
273.403795	8000.091305	10.226893	-0.055653	4.815585
273.564469	8000.148371	10.231898	-0.055683	4.815601
273.463084	8000.137083	10.236903	-0.055664	4.815598
273.517900	8000.206305	10.241907	-0.055674	4.815618
273.444509	8000.198678	10.246912	-0.055660	4.815616
273.402212	8000.124277	10.251917	-0.055652	4.815595
273.519901	8000.172098	10.256922	-0.055673	4.815608
273.375362	8000.087486	10.261927	-0.055646	4.815584
273.414119	8000.119067	10.266931	-0.055653	4.815593
273.519192	8000.163478	10.271936	-0.055672	4.815606
273.496813	8000.109694	10.276941	-0.055668	4.815590
273.593903	8000.144363	10.281946	-0.055686	4.815600
273.548006	8000.125437	10.286951	-0.055677	4.815595
273.439545	8000.152480	10.291955	-0.055657	4.815603
273.497014	8000.122426	10.296960	-0.055667	4.815594
273.592573	8000.100469	10.301965	-0.055685	4.815587
273.684233	8000.152137	10.306970	-0.055701	4.815602
273.653572	8000.121712	10.311975	-0.055695	4.815593
273.715016	8000.146188	10.316979	-0.055707	4.815600
273.947551	8000.151030	10.321984	-0.055750	4.815600
273.678435	8000.104966	10.326989	-0.055699	4.815588
273.862083	8000.139980	10.331994	-0.055733	4.815597
273.856938	8000.184729	10.336999	-0.055732	4.815611
273.734098	8000.150663	10.342003	-0.055709	4.815601
273.666997	8000.142071	10.347008	-0.055696	4.815599
273.823038	8000.123237	10.352013	-0.055725	4.815593
273.581470	8000.155583	10.357018	-0.055680	4.815603
273.591916	8000.177091	10.362023	-0.055682	4.815610
273.508801	8000.132995	10.367027	-0.055666	4.815597
273.705757	8000.100945	10.372032	-0.055702	4.815587
273.616446	8000.135776	10.377037	-0.055685	4.815597
273.624874	8000.164727	10.382042	-0.055687	4.815606
273.721803	8000.140656	10.387047	-0.055704	4.815598
273.769299	8000.138206	10.392051	-0.055713	4.815597
273.823153	8000.167898	10.397056	-0.055723	4.815606
273.849709	8000.085009	10.402061	-0.055728	4.815582
274.075751	8000.126056	10.407066	-0.055769	4.815592
273.836485	8000.144556	10.412071	-0.055725	4.815599
273.626114	8000.156052	10.417075	-0.055685	4.815603
274.030082	8000.238450	10.422080	-0.055760	4.815626
273.656193	8000.096694	10.427085	-0.055690	4.815586
273.773170	8000.145572	10.432090	-0.055712	4.815600
273.598719	8000.111732	10.437095	-0.055679	4.815591
273.764688	8000.108012	10.442099	-0.055710	4.815589
273.827445	8000.116490	10.447104	-0.055721	4.815591
273.681649	8000.129040	10.452109	-0.055694	4.815595
273.820388	8000.180409	10.457114	-0.055719	4.815610
273.571455	8000.101568	10.462119	-0.055673	4.815588
273.716066	8000.122061	10.467123	-0.055699	4.815593
273.937254	8000.142737	10.472128	-0.055740	4.815598
273.818494	8000.095923	10.477133	-0.055718	4.815585
273.986600	8000.147771	10.482138	-0.055749	4.815599
273.905753	8000.189148	10.487143	-0.055734	4.815612
274.041846	8000.143290	10.492147	-0.055759	4.815598
273.854603	8000.186134	10.497152	-0.055724	4.815611
273.593309	8000.128450	10.502157	-0.055675	4.815596
273.815673	8000.187591	10.507162	-0.055716	4.815612
273.663357	8000.139162	10.512167	-0.055687	4.815598
273.781169	8000.106888	10.517171	-0.055709	4.815588
273.811973	8000.127660	10.522176	-0.055715	4.815594
273.728541	8000.136957	10.527181	-0.055699	4.815597
273.882912	8000.168290	10.532186	-0.055727	4.815606
273.919850	8000.135764	10.537191	-0.055734	4.815596
274.081100	8000.155462	10.542195	-0.055764	4.815601
273.912944	8000.186870	10.547200	-0.055732	4.815611
273.876699	8000.127519	10.552205	-0.055725	4.815594
274.027107	8000.168399	10.557210	-0.055753	4.815605
273.923140	8000.161341	10.562215	-0.055733	4.815604
273.745200	8000.128512	10.567219	-0.055700	4.815595
273.920226	8000.186881	10.572224	-0.055732	4.815611
273.880550	8000.164852	10.577229	-0.055725	4.815605
273.908076	8000.186639	10.582234	-0.055730	4.815611
273.830736	8000.161860	10.587239	-0.055715	4.815604
273.873546	8000.135838	10.592243	-0.055723	4.815596
273.971141	8000.116050	10.597248	-0.055741	4.815590
273.865550	8000.094014	10.602253	-0.055721	4.815584
273.970390	8000.152305	10.607258	-0.055740	4.815601
273.954190	8000.152019	10.612263	-0.055737	4.815601
273.695800	8000.132829	10.617267	-0.055688	4.815596
273.572556	8000.161767	10.622272	-0.055665	4.815606
273.961127	8000.077311	10.627277	-0.055737	4.815579
273.961120	8000.113599	10.632282	-0.055737	4.815590
273.750034	8000.097317	10.637287	-0.055697	4.815586
273.952480	8000.120891	10.642291	-0.055735	4.815592
273.984531	8000.152363	10.647296	-0.055741	4.815601
273.780271	8000.139396	10.652301	-0.055702	4.815598
273.907334	8000.151060	10.657306	-0.055726	4.815601
274.159670	8000.134866	10.662311	-0.055772	4.815595
273.893268	8000.121952	10.667315	-0.055723	4.815592
274.105471	8000.164909	10.672320	-0.055762	4.815604
274.271971	8000.159061	10.677325	-0.055793	4.815601
274.168259	8000.198997	10.682330	-0.055773	4.815614
273.950646	8000.161249	10.687335	-0.055732	4.815604
274.037343	8000.141283	10.692339	-0.055748	4.815597
274.123782	8000.180051	10.697344	-0.055764	4.815608
273.884695	8000.109913	10.702349	-0.055719	4.815589
273.972968	8000.156187	10.707354	-0.055735	4.815602
274.108500	8000.120999	10.712359	-0.055760	4.815591
273.968670	8000.135782	10.717363	-0.055734	4.815596
274.127457	8000.125537	10.722368	-0.055763	4.815592
274.207968	8000.121489	10.727373	-0.055778	4.815591
274.284415	8000.170774	10.732378	-0.055792	4.815605
273.935215	8000.093499	10.737383	-0.055727	4.815584
274.066578	8000.104165	10.742387	-0.055751	4.815587
274.063417	8000.128655	10.747392	-0.055750	4.815594
273.947055	8000.085084	10.752397	-0.055728	4.815582
274.165998	8000.140966	10.757402	-0.055769	4.815597
274.190500	8000.136004	10.762407	-0.055773	4.815595
274.155853	8000.099106	10.767411	-0.055766	4.815585
274.173507	8000.134616	10.772416	-0.055770	4.815595
274.074704	8000.096671	10.777421	-0.055751	4.815584
274.133079	8000.174495	10.782426	-0.055762	4.815607
274.021680	8000.157704	10.787431	-0.055741	4.815602
274.062952	8000.159424	10.792435	-0.055748	4.815603
274.071515	8000.120027	10.797440	-0.055749	4.815591
274.002468	8000.113539	10.802445	-0.055736	4.815590
273.901742	8000.160999	10.807450	-0.055717	4.815604
274.058378	8000.121884	10.812455	-0.055746	4.815592
273.957019	8000.118072	10.817459	-0.055727	4.815591
273.954033	8000.122273	10.822464	-0.055726	4.815592
274.017067	8000.111533	10.827469	-0.055738	4.815589
274.056652	8000.153808	10.832474	-0.055745	4.815601
274.043501	8000.157843	10.837479	-0.055742	4.815602
273.905542	8000.161978	10.842483	-0.055716	4.815604
273.945665	8000.177562	10.847488	-0.055723	4.815609
273.917538	8000.119412	10.852493	-0.055718	4.815592
274.186977	8000.141943	10.857498	-0.055768	4.815597
274.044123	8000.167357	10.862503	-0.055741	4.815605
274.023645	8000.109331	10.867507	-0.055737	4.815588
274.111891	8000.163080	10.872512	-0.055753	4.815604
273.931961	8000.130219	10.877517	-0.055719	4.815595
274.119722	8000.142873	10.882522	-0.055754	4.815598
274.258633	8000.130168	10.887527	-0.055780	4.815593
274.135647	8000.130274	10.892531	-0.055757	4.815594
274.085253	8000.131566	10.897536	-0.055747	4.815595
274.130428	8000.095971	10.902541	-0.055755	4.815584
274.178706	8000.154408	10.907546	-0.055764	4.815601
274.172666	8000.132928	10.912551	-0.055762	4.815595
274.304673	8000.124382	10.917555	-0.055787	4.815592
274.297443	8000.135990	10.922560	-0.055785	4.815595
274.224392	8000.098465	10.927565	-0.055771	4.815584
274.348375	8000.159205	10.932570	-0.055794	4.815601
274.258086	8000.113923	10.937575	-0.055777	4.815589
273.972721	8000.107108	10.942579	-0.055724	4.815588
274.193876	8000.114967	10.947584	-0.055765	4.815589
274.000274	8000.080815	10.952589	-0.055728	4.815580
274.054847	8000.152169	10.957594	-0.055738	4.815601
274.182561	8000.127533	10.962599	-0.055762	4.815593
274.200499	8000.134212	10.967603	-0.055765	4.815595
274.092606	8000.111070	10.972608	-0.055745	4.815589
274.205785	8000.100081	10.977613	-0.055765	4.815585
274.226226	8000.147383	10.982618	-0.055769	4.815599
274.149818	8000.125823	10.987623	-0.055755	4.815593
273.975662	8000.097328	10.992627	-0.055722	4.815585
274.199616	8000.143680	10.997632	-0.055763	4.815598
274.137085	8000.109531	11.002637	-0.055751	4.815588
274.050416	8000.137997	11.007642	-0.055735	4.815597
274.063687	8000.108289	11.012647	-0.055737	4.815588
274.056880	8000.118836	11.017651	-0.055736	4.815591
273.979623	8000.160272	11.022656	-0.055721	4.815604
273.968564	8000.113080	11.027661	-0.055719	4.815590
274.125672	8000.156205	11.032666	-0.055748	4.815602
274.175469	8000.147384	11.037671	-0.055757	4.815599
273.944069	8000.148926	11.042675	-0.055714	4.815601
274.153835	8000.176891	11.047680	-0.055752	4.815608
274.013301	8000.093411	11.052685	-0.055726	4.815584
274.139529	8000.148847	11.057690	-0.055749	4.815600
274.399309	8000.124231	11.062695	-0.055797	4.815591
274.294736	8000.110755	11.067699	-0.055778	4.815588
274.108496	8000.121577	11.072704	-0.055743	4.815592
274.301028	8000.095863	11.077709	-0.055778	4.815583
274.344460	8000.146744	11.082714	-0.055786	4.815598
274.299372	8000.128899	11.087719	-0.055777	4.815593
274.025275	8000.083821	11.092723	-0.055726	4.815581
274.369491	8000.119321	11.097728	-0.055790	4.815590
274.248028	8000.088482	11.102733	-0.055767	4.815582
274.142299	8000.135860	11.107738	-0.055747	4.815596
274.249194	8000.146127	11.112743	-0.055767	4.815598
274.365718	8000.129852	11.117747	-0.055788	4.815593
274.257874	8000.212440	11.122752	-0.055768	4.815618
274.248324	8000.153524	11.127757	-0.055766	4.815601
274.554839	8000.137147	11.132762	-0.055823	4.815594
274.397015	8000.135617	11.137767	-0.055793	4.815595
274.281955	8000.124105	11.142771	-0.055771	4.815592
274.342849	8000.148573	11.147776	-0.055783	4.815599
274.277832	8000.075936	11.152781	-0.055770	4.815578
274.240263	8000.110544	11.157786	-0.055763	4.815588
274.336526	8000.179376	11.162791	-0.055781	4.815608
274.309757	8000.122315	11.167795	-0.055775	4.815591
274.464484	8000.156858	11.172800	-0.055804	4.815601
274.215271	8000.143156	11.177805	-0.055757	4.815598
274.421575	8000.119803	11.182810	-0.055796	4.815590
274.417089	8000.118640	11.187815	-0.055794	4.815590
274.336511	8000.098080	11.192819	-0.055779	4.815584
274.499573	8000.124215	11.197824	-0.055809	4.815591
274.490255	8000.141129	11.202829	-0.055807	4.815596
274.367538	8000.139104	11.207834	-0.055784	4.815596
274.275449	8000.091657	11.212839	-0.055767	4.815582
274.357360	8000.114332	11.217843	-0.055782	4.815589
274.493315	8000.160316	11.222848	-0.055807	4.815601
274.308190	8000.092127	11.227853	-0.055772	4.815582
274.390704	8000.129763	11.232858	-0.055787	4.815593
274.347734	8000.113020	11.237863	-0.055779	4.815588
274.218805	8000.104486	11.242867	-0.055755	4.815587
274.444607	8000.094267	11.247872	-0.055797	4.815582
274.376829	8000.099547	11.252877	-0.055784	4.815584
274.482366	8000.101248	11.257882	-0.055803	4.815584
274.442933	8000.121942	11.262887	-0.055796	4.815591
274.170135	8000.109991	11.267891	-0.055744	4.815588
274.355258	8000.127943	11.272896	-0.055779	4.815593
274.194488	8000.077239	11.277901	-0.055749	4.815579
274.561746	8000.131270	11.282906	-0.055817	4.815593
274.607269	8000.115972	11.287911	-0.055825	4.815588
274.217214	8000.102108	11.292915	-0.055752	4.815586
274.263269	8000.092158	11.297920	-0.055760	4.815583
274.253292	8000.072751	11.302925	-0.055758	4.815577
274.360214	8000.090494	11.307930	-0.055778	4.815582
274.320848	8000.099441	11.312935	-0.055770	4.815585
274.612217	8000.098836	11.317939	-0.055824	4.815583
274.595669	8000.138059	11.322944	-0.055821	4.815595
274.215741	8000.082709	11.327949	-0.055750	4.815580
274.409123	8000.128563	11.332954	-0.055786	4.815593
274.450230	8000.147367	11.337959	-0.055793	4.815598
274.269218	8000.101672	11.342963	-0.055759	4.815586
274.278317	8000.096460	11.347968	-0.055761	4.815584
274.385489	8000.117411	11.352973	-0.055780	4.815590
274.402787	8000.157186	11.357978	-0.055783	4.815601
274.255285	8000.125922	11.362983	-0.055756	4.815593
274.308259	8000.092590	11.367987	-0.055765	4.815583
274.491623	8000.119056	11.372992	-0.055799	4.815590
274.270241	8000.102606	11.377997	-0.055758	4.815586
274.467748	8000.137847	11.383002	-0.055794	4.815595
274.593893	8000.119593	11.388007	-0.055817	4.815589
274.316088	8000.086202	11.393011	-0.055765	4.815581
274.351638	8000.135887	11.398016	-0.055772	4.815595
274.381686	8000.095773	11.403021	-0.055777	4.815583
274.641897	8000.142718	11.408026	-0.055825	4.815596
274.400613	8000.116330	11.413031	-0.055780	4.815589
274.465979	8000.105628	11.418035	-0.055792	4.815586
274.755836	8000.132765	11.423040	-0.055846	4.815592
274.492390	8000.113491	11.428045	-0.055797	4.815588
274.294796	8000.134807	11.433050	-0.055760	4.815595
274.565462	8000.098621	11.438055	-0.055810	4.815583
274.399158	8000.102293	11.443059	-0.055778	4.815585
274.414461	8000.143104	11.448064	-0.055781	4.815597
274.301475	8000.115606	11.453069	-0.055760	4.815590
274.487065	8000.127158	11.458074	-0.055794	4.815592
274.449504	8000.197009	11.463079	-0.055787	4.815613
274.241292	8000.115627	11.468083	-0.055748	4.815590
274.609156	8000.138698	11.473088	-0.055816	4.815595
274.580119	8000.138202	11.478093	-0.055810	4.815595
274.448694	8000.139239	11.483098	-0.055786	4.815596
274.720469	8000.153266	11.488103	-0.055836	4.815599
274.436286	8000.100546	11.493107	-0.055783	4.815585
274.526816	8000.130838	11.498112	-0.055800	4.815593
274.526868	8000.075283	11.503117	-0.055799	4.815577
274.603566	8000.090396	11.508122	-0.055813	4.815581
274.470101	8000.090332	11.513127	-0.055788	4.815582
274.295074	8000.086386	11.518131	-0.055755	4.815581
274.385124	8000.126281	11.523136	-0.055772	4.815592
274.452511	8000.122019	11.528141	-0.055784	4.815591
274.328844	8000.129591	11.533146	-0.055761	4.815594
274.377585	8000.092986	11.538151	-0.055770	4.815583
274.439145	8000.084357	11.543155	-0.055781	4.815580
274.489365	8000.111854	11.548160	-0.055790	4.815588
274.487247	8000.122478	11.553165	-0.055789	4.815591
274.524002	8000.142280	11.558170	-0.055796	4.815596
274.551648	8000.129894	11.563175	-0.055801	4.815593
274.265321	8000.098499	11.568179	-0.055747	4.815585
274.483025	8000.111643	11.573184	-0.055788	4.815588
274.406374	8000.077263	11.578189	-0.055773	4.815578
274.346466	8000.109371	11.583194	-0.055762	4.815588
274.447287	8000.096043	11.588199	-0.055780	4.815583
274.708699	8000.106696	11.593203	-0.055829	4.815585
274.531774	8000.158253	11.598208	-0.055796	4.815601
274.441848	8000.106569	11.603213	-0.055779	4.815587
274.688604	8000.150090	11.608218	-0.055824	4.815598
274.618465	8000.156399	11.613223	-0.055811	4.815600
274.300481	8000.112740	11.618227	-0.055751	4.815589
274.656755	8000.138826	11.623232	-0.055818	4.815595
274.571750	8000.095766	11.628237	-0.055801	4.815583
274.638194	8000.151295	11.633242	-0.055814	4.815599
274.609169	8000.132644	11.638247	-0.055808	4.815593
274.677906	8000.109181	11.643251	-0.055821	4.815586
274.708205	8000.147033	11.648256	-0.055826	4.815597
274.598348	8000.131335	11.653261	-0.055805	4.815593
274.524335	8000.151464	11.658266	-0.055791	4.815599
274.499980	8000.145705	11.663271	-0.055786	4.815598
274.545058	8000.107972	11.668275	-0.055795	4.815587
274.840851	8000.130935	11.673280	-0.055849	4.815592
274.725930	8000.124765	11.678285	-0.055828	4.815591
274.711571	8000.144801	11.683290	-0.055825	4.815596
274.728121	8000.129030	11.688295	-0.055828	4.815592
274.722193	8000.120368	11.693299	-0.055826	4.815589
274.780220	8000.177896	11.698304	-0.055837	4.815606
274.672847	8000.110975	11.703309	-0.055817	4.815587
274.681523	8000.129250	11.708314	-0.055818	4.815592
274.648935	8000.110541	11.713319	-0.055812	4.815587
274.580412	8000.104061	11.718323	-0.055799	4.815585
274.589488	8000.120207	11.723328	-0.055800	4.815590
274.557989	8000.097244	11.728333	-0.055794	4.815583
274.545666	8000.141876	11.733338	-0.055791	4.815596
274.771083	8000.122039	11.738343	-0.055833	4.815590
274.553321	8000.104579	11.743347	-0.055792	4.815586
274.680627	8000.181393	11.748352	-0.055816	4.815607
274.650628	8000.118940	11.753357	-0.055810	4.815589
274.819995	8000.124887	11.758362	-0.055841	4.815590
274.887887	8000.133449	11.763367	-0.055854	4.815592
274.809282	8000.103309	11.768371	-0.055839	4.815584
274.847639	8000.137021	11.773376	-0.055846	4.815594
274.838766	8000.124039	11.778381	-0.055844	4.815590
274.839497	8000.114417	11.783386	-0.055844	4.815587
274.545973	8000.088245	11.788391	-0.055789	4.815581
274.696067	8000.099217	11.793395	-0.055816	4.815583
274.700693	8000.129174	11.798400	-0.055817	4.815592
274.628945	8000.138661	11.803405	-0.055804	4.815595
274.545393	8000.144751	11.808410	-0.055788	4.815597
274.620784	8000.121397	11.813415	-0.055801	4.815590
274.503479	8000.100237	11.818419	-0.055779	4.815585
274.640273	8000.243420	11.823424	-0.055805	4.815626
274.680983	8000.128722	11.828429	-0.055812	4.815592
274.791957	8000.148668	11.833434	-0.055832	4.815597
274.919390	8000.151795	11.838439	-0.055856	4.815598
274.830879	8000.107609	11.843443	-0.055839	4.815585
274.834207	8000.171720	11.848448	-0.055840	4.815604
274.752743	8000.165029	11.853453	-0.055824	4.815602
274.573064	8000.150326	11.858458	-0.055790	4.815599
274.594987	8000.126099	11.863463	-0.055794	4.815592
274.487244	8000.120047	11.868467	-0.055774	4.815591
274.764187	8000.221732	11.873472	-0.055825	4.815619
274.881265	8000.167019	11.878477	-0.055847	4.815602
274.680691	8000.163723	11.883482	-0.055809	4.815602
274.696900	8000.147946	11.888487	-0.055812	4.815598
274.783687	8000.117302	11.893491	-0.055828	4.815588
274.796483	8000.148460	11.898496	-0.055830	4.815597
274.702059	8000.116994	11.903501	-0.055812	4.815589
274.621696	8000.117797	11.908506	-0.055797	4.815589
274.688813	8000.145570	11.913511	-0.055809	4.815597
274.597008	8000.106671	11.918515	-0.055792	4.815586
274.601425	8000.159051	11.923520	-0.055792	4.815601
274.724536	8000.102301	11.928525	-0.055815	4.815584
274.619233	8000.125124	11.933530	-0.055795	4.815592
274.551448	8000.132540	11.938535	-0.055782	4.815594
274.680176	8000.117532	11.943539	-0.055806	4.815589
274.666049	8000.131163	11.948544	-0.055803	4.815593
274.637517	8000.091161	11.953549	-0.055798	4.815582
274.563621	8000.115564	11.958554	-0.055784	4.815589
274.933989	8000.119453	11.963559	-0.055852	4.815588
274.814816	8000.092922	11.968563	-0.055830	4.815581
274.800753	8000.125778	11.973568	-0.055827	4.815591
274.658310	8000.101004	11.978573	-0.055800	4.815584
274.734039	8000.123578	11.983578	-0.055814	4.815591
274.747523	8000.115232	11.988583	-0.055816	4.815588
274.694232	8000.090846	11.993587	-0.055806	4.815581
274.916868	8000.124362	11.998592	-0.055847	4.815590
274.771462	8000.115558	12.003597	-0.055820	4.815588
274.748342	8000.138655	12.008602	-0.055816	4.815595
274.735061	8000.112785	12.013607	-0.055813	4.815587
274.709871	8000.090993	12.018611	-0.055808	4.815581
274.734018	8000.112725	12.023616	-0.055812	4.815587
274.845501	8000.092096	12.028621	-0.055833	4.815581
274.800395	8000.102017	12.033626	-0.055824	4.815584
274.850540	8000.106018	12.038631	-0.055833	4.815585
274.777818	8000.101605	12.043635	-0.055819	4.815584
274.876918	8000.145920	12.048640	-0.055838	4.815596
274.805416	8000.114828	12.053645	-0.055824	4.815588
274.681087	8000.117049	12.058650	-0.055801	4.815589
274.715469	8000.148560	12.063655	-0.055807	4.815598
274.524270	8000.094155	12.068659	-0.055771	4.815583
274.732001	8000.142378	12.073664	-0.055809	4.815596
274.711231	8000.122794	12.078669	-0.055805	4.815591
275.001927	8000.120043	12.083674	-0.055859	4.815588
274.907001	8000.149442	12.088679	-0.055841	4.815597
274.489140	8000.093473	12.093683	-0.055763	4.815583
274.803305	8000.159454	12.098688	-0.055821	4.815601
274.717032	8000.156956	12.103693	-0.055805	4.815601
274.771009	8000.136456	12.108698	-0.055815	4.815594
274.801825	8000.176452	12.113703	-0.055820	4.815606
274.641852	8000.100129	12.118707	-0.055790	4.815584
274.674794	8000.198899	12.123712	-0.055796	4.815613
274.636136	8000.163003	12.128717	-0.055789	4.815603
274.693833	8000.120136	12.133722	-0.055799	4.815590
274.864981	8000.118637	12.138727	-0.055831	4.815589
274.594028	8000.096037	12.143731	-0.055780	4.815583
274.951227	8000.134953	12.148736	-0.055846	4.815593
274.956077	8000.108311	12.153741	-0.055847	4.815585
274.794036	8000.121664	12.158746	-0.055817	4.815590
274.961655	8000.117971	12.163751	-0.055848	4.815588
274.781493	8000.136367	12.168755	-0.055814	4.815594
274.896382	8000.145697	12.173760	-0.055835	4.815596
274.984463	8000.111870	12.178765	-0.055851	4.815586
275.088327	8000.142380	12.183770	-0.055870	4.815595
275.121029	8000.159980	12.188775	-0.055876	4.815600
274.867695	8000.133395	12.193779	-0.055829	4.815593
274.966581	8000.148871	12.198784	-0.055847	4.815597
274.805479	8000.096025	12.203789	-0.055817	4.815582
274.771817	8000.099725	12.208794	-0.055810	4.815584
274.793370	8000.128891	12.213799	-0.055814	4.815592
274.874992	8000.084279	12.218803	-0.055829	4.815579
274.831245	8000.147621	12.223808	-0.055820	4.815597
275.014784	8000.116421	12.228813	-0.055854	4.815587
274.990646	8000.108529	12.233818	-0.055850	4.815585
274.833376	8000.158271	12.238823	-0.055820	4.815601
274.719911	8000.125426	12.243827	-0.055799	4.815592
274.999844	8000.166285	12.248832	-0.055851	4.815602
274.770139	8000.095231	12.253837	-0.055808	4.815582
274.806628	8000.101145	12.258842	-0.055814	4.815584
274.792071	8000.125449	12.263847	-0.055811	4.815591
274.825667	8000.112092	12.268851	-0.055817	4.815587
275.011310	8000.138597	12.273856	-0.055852	4.815594
274.923742	8000.154233	12.278861	-0.055835	4.815599
274.914050	8000.135898	12.283866	-0.055833	4.815594
274.859348	8000.147799	12.288871	-0.055822	4.815597
274.860554	8000.122166	12.293875	-0.055822	4.815590
274.990787	8000.156309	12.298880	-0.055846	4.815599
274.914712	8000.136890	12.303885	-0.055832	4.815594
275.057481	8000.137063	12.308890	-0.055858	4.815593
274.904841	8000.144161	12.313895	-0.055830	4.815596
274.927112	8000.132756	12.318899	-0.055834	4.815593
274.876299	8000.163944	12.323904	-0.055824	4.815602
274.674034	8000.127513	12.328909	-0.055786	4.815592
274.757988	8000.112842	12.333914	-0.055801	4.815588
274.970928	8000.109889	12.338919	-0.055841	4.815586
274.844671	8000.086447	12.343923	-0.055817	4.815580
274.990072	8000.143265	12.348928	-0.055844	4.815596
274.860978	8000.092010	12.353933	-0.055820	4.815581
274.747659	8000.099750	12.358938	-0.055798	4.815584
274.757502	8000.106297	12.363943	-0.055800	4.815586
274.854846	8000.083301	12.368947	-0.055818	4.815579
275.156687	8000.129858	12.373952	-0.055874	4.815591
274.939100	8000.099585	12.378957	-0.055833	4.815583
274.859612	8000.112149	12.383962	-0.055818	4.815587
275.174481	8000.134355	12.388967	-0.055876	4.815592
275.088788	8000.123323	12.393971	-0.055860	4.815589
275.131055	8000.125059	12.398976	-0.055868	4.815590
275.039891	8000.105394	12.403981	-0.055850	4.815584
274.959187	8000.121142	12.408986	-0.055835	4.815589
275.042168	8000.182282	12.413991	-0.055850	4.815607
274.879224	8000.109114	12.418995	-0.055820	4.815586
274.937887	8000.142089	12.424000	-0.055830	4.815596
274.984170	8000.081948	12.429005	-0.055839	4.815578
274.993216	8000.099162	12.434010	-0.055840	4.815583
274.951534	8000.141179	12.439015	-0.055832	4.815595
274.657572	8000.082960	12.444019	-0.055777	4.815580
274.774856	8000.104076	12.449024	-0.055799	4.815585
274.853189	8000.101061	12.454029	-0.055813	4.815584
274.984253	8000.114927	12.459034	-0.055837	4.815587
275.052365	8000.112813	12.464039	-0.055850	4.815587
275.033332	8000.106073	12.469043	-0.055846	4.815585
275.214346	8000.130366	12.474048	-0.055879	4.815591
274.917813	8000.118028	12.479053	-0.055824	4.815589
274.885865	8000.111077	12.484058	-0.055818	4.815587
275.152725	8000.151723	12.489063	-0.055867	4.815597
274.901034	8000.097397	12.494067	-0.055820	4.815583
275.038415	8000.102822	12.499072	-0.055845	4.815584
274.972130	8000.100651	12.504077	-0.055833	4.815583
275.064351	8000.096795	12.509082	-0.055850	4.815582
275.100238	8000.125126	12.514087	-0.055856	4.815590
275.003138	8000.102160	12.519091	-0.055838	4.815584
275.052995	8000.143535	12.524096	-0.055847	4.815596
275.153315	8000.131268	12.529101	-0.055865	4.815592
274.912106	8000.143328	12.534106	-0.055820	4.815596
275.006899	8000.145922	12.539111	-0.055838	4.815596
274.992670	8000.106153	12.544115	-0.055835	4.815585
275.197441	8000.139378	12.549120	-0.055873	4.815594
274.947599	8000.155568	12.554125	-0.055826	4.815600
274.998937	8000.117938	12.559130	-0.055835	4.815588
275.098509	8000.139833	12.564135	-0.055853	4.815594
275.004897	8000.100904	12.569139	-0.055836	4.815583
275.246530	8000.141139	12.574144	-0.055881	4.815594
275.173958	8000.123913	12.579149	-0.055867	4.815589
274.923019	8000.116590	12.584154	-0.055820	4.815588
275.013889	8000.146887	12.589159	-0.055836	4.815597
274.951800	8000.143716	12.594163	-0.055825	4.815596
274.931778	8000.149776	12.599168	-0.055821	4.815598
275.006305	8000.126407	12.604173	-0.055834	4.815591
275.034774	8000.095879	12.609178	-0.055839	4.815582
274.987632	8000.170914	12.614183	-0.055830	4.815604
274.999530	8000.129436	12.619187	-0.055832	4.815592
275.048594	8000.128079	12.624192	-0.055841	4.815591
274.808036	8000.141218	12.629197	-0.055796	4.815596
274.935825	8000.155030	12.634202	-0.055820	4.815600
274.900049	8000.149084	12.639207	-0.055813	4.815598
274.971069	8000.154494	12.644211	-0.055826	4.815599
275.078982	8000.150894	12.649216	-0.055846	4.815598
275.133030	8000.110104	12.654221	-0.055855	4.815586
275.033225	8000.096705	12.659226	-0.055837	4.815582
275.096120	8000.132954	12.664231	-0.055848	4.815592
274.866491	8000.092872	12.669235	-0.055805	4.815582
275.136192	8000.100457	12.674240	-0.055855	4.815583
274.955199	8000.124180	12.679245	-0.055821	4.815591
274.879483	8000.106903	12.684250	-0.055807	4.815586
275.098845	8000.155317	12.689255	-0.055847	4.815599
275.145004	8000.107991	12.694259	-0.055856	4.815585
275.244283	8000.130949	12.699264	-0.055874	4.815591
275.110355	8000.151169	12.704269	-0.055849	4.815598
275.125756	8000.134311	12.709274	-0.055851	4.815593
275.147253	8000.164543	12.714279	-0.055855	4.815601
275.134735	8000.160045	12.719283	-0.055853	4.815600
275.161060	8000.158318	12.724288	-0.055857	4.815600
275.102286	8000.135977	12.729293	-0.055846	4.815593
274.978522	8000.118983	12.734298	-0.055823	4.815589
275.183835	8000.161829	12.739303	-0.055861	4.815601
275.083168	8000.124920	12.744307	-0.055842	4.815590
275.063405	8000.154479	12.749312	-0.055838	4.815599
275.024564	8000.155959	12.754317	-0.055830	4.815600
275.215105	8000.130213	12.759322	-0.055866	4.815591
275.231255	8000.198806	12.764327	-0.055868	4.815611
275.218344	8000.156922	12.769331	-0.055866	4.815599
275.164162	8000.154948	12.774336	-0.055855	4.815599
275.361080	8000.133578	12.779341	-0.055892	4.815592
275.012884	8000.099036	12.784346	-0.055827	4.815583
275.147649	8000.140730	12.789351	-0.055851	4.815595
275.132994	8000.088138	12.794355	-0.055848	4.815579
275.107940	8000.125087	12.799360	-0.055844	4.815590
274.879837	8000.127749	12.804365	-0.055801	4.815592
275.182359	8000.129462	12.809370	-0.055857	4.815591
275.321443	8000.202198	12.814375	-0.055883	4.815612
275.086450	8000.107562	12.819379	-0.055839	4.815585
275.269158	8000.104115	12.824384	-0.055872	4.815583
275.181097	8000.156054	12.829389	-0.055856	4.815599
275.146084	8000.134102	12.834394	-0.055849	4.815593
275.161589	8000.162100	12.839399	-0.055852	4.815601
275.274434	8000.111590	12.844403	-0.055872	4.815586
275.133496	8000.113540	12.849408	-0.055846	4.815587
275.253018	8000.116537	12.854413	-0.055868	4.815587
275.168335	8000.086298	12.859418	-0.055852	4.815579
275.166158	8000.128960	12.864423	-0.055851	4.815591
274.872088	8000.101710	12.869427	-0.055796	4.815585
275.123204	8000.119671	12.874432	-0.055843	4.815589
275.092720	8000.151191	12.879437	-0.055837	4.815598
275.168032	8000.142787	12.884442	-0.055851	4.815595
275.205222	8000.188228	12.889447	-0.055857	4.815608
275.147997	8000.142417	12.894451	-0.055846	4.815595
275.107209	8000.123574	12.899456	-0.055839	4.815590
275.101413	8000.114914	12.904461	-0.055837	4.815587
275.250283	8000.123730	12.909466	-0.055865	4.815589
275.445237	8000.192039	12.914471	-0.055901	4.815608
275.278610	8000.123082	12.919475	-0.055869	4.815589
275.341480	8000.166806	12.924480	-0.055881	4.815601
275.376408	8000.132111	12.929485	-0.055887	4.815591
275.261940	8000.131288	12.934490	-0.055866	4.815592
275.481126	8000.177565	12.939495	-0.055906	4.815604
275.371022	8000.180017	12.944499	-0.055885	4.815605
275.337154	8000.137791	12.949504	-0.055879	4.815593
275.321174	8000.186636	12.954509	-0.055876	4.815607
275.375668	8000.138377	12.959514	-0.055886	4.815593
275.446737	8000.197187	12.964519	-0.055899	4.815610
275.324189	8000.147105	12.969523	-0.055875	4.815596
275.366266	8000.158450	12.974528	-0.055883	4.815599
275.179962	8000.157523	12.979533	-0.055848	4.815600
275.125372	8000.174765	12.984538	-0.055838	4.815605
275.325259	8000.226066	12.989543	-0.055875	4.815619
275.328511	8000.147067	12.994547	-0.055875	4.815596
275.204556	8000.132206	12.999552	-0.055852	4.815592
275.341136	8000.082083	13.004557	-0.055877	4.815577
275.437698	8000.110338	13.009562	-0.055895	4.815585
275.481777	8000.148415	13.014567	-0.055903	4.815596
275.464245	8000.161991	13.019571	-0.055899	4.815600
275.380995	8000.163814	13.024576	-0.055883	4.815601
275.463853	8000.133106	13.029581	-0.055899	4.815591
275.414263	8000.144022	13.034586	-0.055889	4.815595
275.328885	8000.140471	13.039591	-0.055873	4.815594
275.590711	8000.122296	13.044595	-0.055921	4.815587
275.304194	8000.145364	13.049600	-0.055868	4.815596
275.389065	8000.190515	13.054605	-0.055883	4.815608
275.372064	8000.142157	13.059610	-0.055880	4.815594
275.561475	8000.214647	13.064615	-0.055915	4.815615
275.245796	8000.133644	13.069619	-0.055856	4.815592
275.356056	8000.140763	13.074624	-0.055876	4.815594
275.453733	8000.187191	13.079629	-0.055894	4.815607
275.220185	8000.128889	13.084634	-0.055850	4.815591
275.356316	8000.191965	13.089639	-0.055876	4.815609
275.417453	8000.139543	13.094643	-0.055887	4.815593
275.425631	8000.157810	13.099648	-0.055888	4.815599
275.325750	8000.135866	13.104653	-0.055869	4.815593
275.378657	8000.121757	13.109658	-0.055879	4.815588
275.388624	8000.190249	13.114663	-0.055880	4.815608
275.216774	8000.116935	13.119667	-0.055848	4.815588
275.238300	8000.101245	13.124672	-0.055852	4.815583
275.332741	8000.107037	13.129677	-0.055869	4.815584
275.330986	8000.103783	13.134682	-0.055869	4.815583
275.375990	8000.162167	13.139687	-0.055877	4.815600
275.293437	8000.114874	13.144691	-0.055861	4.815587
275.683089	8000.162866	13.149696	-0.055933	4.815599
275.568112	8000.195142	13.154701	-0.055912	4.815609
275.487299	8000.129722	13.159706	-0.055896	4.815590
275.533878	8000.202016	13.164711	-0.055905	4.815611
275.503730	8000.204706	13.169715	-0.055899	4.815612
275.453152	8000.183567	13.174720	-0.055889	4.815606
275.426698	8000.178841	13.179725	-0.055884	4.815605
275.308090	8000.125620	13.184730	-0.055862	4.815590
275.459329	8000.161175	13.189735	-0.055890	4.815600
275.370440	8000.120187	13.194739	-0.055873	4.815588
275.396727	8000.136614	13.199744	-0.055878	4.815593
275.421593	8000.125250	13.204749	-0.055882	4.815589
275.284741	8000.112315	13.209754	-0.055856	4.815586
275.412654	8000.180596	13.214759	-0.055880	4.815606
275.328690	8000.139688	13.219763	-0.055864	4.815594
275.210266	8000.146277	13.224768	-0.055842	4.815596
275.398105	8000.136507	13.229773	-0.055876	4.815593
275.311828	8000.120125	13.234778	-0.055860	4.815588
275.503770	8000.173432	13.239783	-0.055896	4.815603
275.258486	8000.137366	13.244787	-0.055850	4.815594
275.425076	8000.158220	13.249792	-0.055880	4.815599
275.536439	8000.186716	13.254797	-0.055901	4.815607
275.531380	8000.124669	13.259802	-0.055900	4.815589
275.527770	8000.127792	13.264807	-0.055899	4.815590
275.411232	8000.134412	13.269811	-0.055877	4.815592
275.401768	8000.155595	13.274816	-0.055875	4.815598
275.454874	8000.159645	13.279821	-0.055885	4.815599
275.374884	8000.098510	13.284826	-0.055869	4.815582
275.381412	8000.154130	13.289831	-0.055870	4.815598
275.104639	8000.110075	13.294835	-0.055819	4.815587
275.408650	8000.135308	13.299840	-0.055875	4.815592
275.437251	8000.201968	13.304845	-0.055880	4.815612
275.353021	8000.132220	13.309850	-0.055864	4.815592
275.482426	8000.140719	13.314855	-0.055888	4.815594
275.563342	8000.148427	13.319859	-0.055903	4.815596
275.382240	8000.143312	13.324864	-0.055869	4.815595
275.448433	8000.158255	13.329869	-0.055881	4.815599
275.636796	8000.096162	13.334874	-0.055916	4.815580
275.579096	8000.163549	13.339879	-0.055905	4.815600
275.367101	8000.152590	13.344883	-0.055865	4.815598
275.752102	8000.152447	13.349888	-0.055936	4.815596
275.648569	8000.208406	13.354893	-0.055917	4.815613
275.557094	8000.187667	13.359898	-0.055900	4.815607
275.541440	8000.248265	13.364903	-0.055896	4.815625
275.561407	8000.169538	13.369907	-0.055900	4.815602
275.430970	8000.195154	13.374912	-0.055875	4.815610
275.425604	8000.190773	13.379917	-0.055874	4.815609
275.426207	8000.165130	13.384922	-0.055874	4.815601
275.409299	8000.164832	13.389927	-0.055871	4.815601
275.348318	8000.167019	13.394931	-0.055859	4.815602
275.351986	8000.156377	13.399936	-0.055859	4.815599
275.623064	8000.167190	13.404941	-0.055910	4.815601
275.566771	8000.154501	13.409946	-0.055899	4.815597
275.503357	8000.185483	13.414951	-0.055887	4.815607
275.392047	8000.150537	13.419955	-0.055866	4.815597
275.654709	8000.193252	13.424960	-0.055915	4.815608
275.450296	8000.186688	13.429965	-0.055876	4.815607
275.386784	8000.148250	13.434970	-0.055864	4.815596
275.557693	8000.185194	13.439975	-0.055896	4.815606
275.434082	8000.161795	13.444979	-0.055872	4.815600
275.577114	8000.199352	13.449984	-0.055899	4.815611
275.697874	8000.177807	13.454989	-0.055921	4.815604
275.474401	8000.137825	13.459994	-0.055879	4.815593
275.342370	8000.124968	13.464999	-0.055854	4.815590
275.622849	8000.196808	13.470003	-0.055906	4.815610
275.818435	8000.181825	13.475008	-0.055943	4.815604
275.411988	8000.135651	13.480013	-0.055867	4.815593
275.476642	8000.126005	13.485018	-0.055878	4.815590
275.643240	8000.159675	13.490023	-0.055909	4.815599
275.586577	8000.148049	13.495027	-0.055898	4.815596
275.676890	8000.165521	13.500032	-0.055915	4.815600
275.672059	8000.202800	13.505037	-0.055914	4.815611
275.716882	8000.162927	13.510042	-0.055922	4.815599
275.648296	8000.144698	13.515047	-0.055909	4.815594
275.732482	8000.153527	13.520051	-0.055924	4.815596
275.587895	8000.187456	13.525056	-0.055897	4.815607
275.509956	8000.161598	13.530061	-0.055882	4.815600
275.522509	8000.127606	13.535066	-0.055884	4.815590
275.833859	8000.151892	13.540071	-0.055942	4.815596
275.576988	8000.080393	13.545075	-0.055894	4.815576
275.679427	8000.151463	13.550080	-0.055913	4.815596
275.621989	8000.144095	13.555085	-0.055902	4.815594
275.432919	8000.117491	13.560090	-0.055867	4.815587
275.679616	8000.193052	13.565095	-0.055912	4.815608
275.601071	8000.153301	13.570099	-0.055897	4.815597
275.584699	8000.172235	13.575104	-0.055894	4.815603
275.740051	8000.207858	13.580109	-0.055923	4.815612
275.612798	8000.139543	13.585114	-0.055899	4.815593
275.641544	8000.164555	13.590119	-0.055904	4.815600
275.582935	8000.125129	13.595123	-0.055893	4.815589
275.512844	8000.125031	13.600128	-0.055879	4.815589
275.655502	8000.209573	13.605133	-0.055906	4.815613
275.497034	8000.137545	13.610138	-0.055876	4.815593
275.731455	8000.119991	13.615143	-0.055919	4.815587
275.577995	8000.114260	13.620147	-0.055891	4.815586
275.523514	8000.137912	13.625152	-0.055880	4.815593
275.481282	8000.142541	13.630157	-0.055872	4.815595
275.447563	8000.102454	13.635162	-0.055866	4.815583
275.575539	8000.137629	13.640167	-0.055889	4.815593
275.657731	8000.132541	13.645171	-0.055904	4.815591
275.685908	8000.147932	13.650176	-0.055909	4.815595
275.728396	8000.131516	13.655181	-0.055917	4.815590
275.635274	8000.094730	13.660186	-0.055899	4.815580
275.564435	8000.181127	13.665191	-0.055886	4.815606
275.622489	8000.253608	13.670195	-0.055897	4.815626
275.497059	8000.188527	13.675200	-0.055873	4.815608
275.402953	8000.223280	13.680205	-0.055855	4.815619
275.513815	8000.140698	13.685210	-0.055875	4.815594
275.678769	8000.164730	13.690215	-0.055906	4.815600
275.505426	8000.121294	13.695219	-0.055873	4.815588
275.567101	8000.124416	13.700224	-0.055885	4.815589
275.661587	8000.177200	13.705229	-0.055902	4.815604
275.584826	8000.099030	13.710234	-0.055887	4.815582
275.535457	8000.129174	13.715239	-0.055878	4.815591
275.608461	8000.099373	13.720243	-0.055891	4.815582
275.768330	8000.146817	13.725248	-0.055921	4.815595
275.768881	8000.188456	13.730253	-0.055921	4.815607
275.633919	8000.144579	13.735258	-0.055895	4.815595
275.867124	8000.167589	13.740263	-0.055939	4.815600
275.809020	8000.148463	13.745267	-0.055927	4.815595
275.709133	8000.158558	13.750272	-0.055909	4.815598
275.688105	8000.160329	13.755277	-0.055904	4.815599
275.565235	8000.119854	13.760282	-0.055881	4.815588
275.586612	8000.131929	13.765287	-0.055885	4.815591
275.753180	8000.121811	13.770291	-0.055916	4.815587
275.613899	8000.136603	13.775296	-0.055890	4.815592
275.823995	8000.167779	13.780301	-0.055929	4.815601
275.795542	8000.165157	13.785306	-0.055923	4.815600
275.763036	8000.145381	13.790311	-0.055917	4.815594
275.645986	8000.096457	13.795315	-0.055895	4.815581
275.631066	8000.104736	13.800320	-0.055892	4.815583
275.703123	8000.105890	13.805325	-0.055905	4.815583
275.650696	8000.118897	13.810330	-0.055895	4.815587
275.650918	8000.194705	13.815335	-0.055895	4.815609
275.517742	8000.246976	13.820339	-0.055870	4.815625
275.748143	8000.157802	13.825344	-0.055912	4.815598
275.651912	8000.178637	13.830349	-0.055894	4.815605
275.538435	8000.119091	13.835354	-0.055873	4.815588
275.702911	8000.160203	13.840359	-0.055903	4.815599
275.497262	8000.094880	13.845363	-0.055864	4.815581
275.700154	8000.140891	13.850368	-0.055902	4.815593
275.723006	8000.173282	13.855373	-0.055906	4.815603
275.532305	8000.096456	13.860378	-0.055870	4.815581
275.617202	8000.126655	13.865383	-0.055886	4.815590
275.501502	8000.125813	13.870387	-0.055864	4.815590
275.594966	8000.126249	13.875392	-0.055881	4.815590
275.548939	8000.144700	13.880397	-0.055872	4.815595
275.650243	8000.120700	13.885402	-0.055891	4.815588
275.636127	8000.138604	13.890407	-0.055888	4.815593
275.557552	8000.137299	13.895411	-0.055873	4.815593
275.577489	8000.126924	13.900416	-0.055877	4.815590
275.737889	8000.142337	13.905421	-0.055906	4.815594
275.745970	8000.136039	13.910426	-0.055908	4.815592
275.645783	8000.156809	13.915431	-0.055889	4.815598
275.640787	8000.143890	13.920435	-0.055888	4.815595
275.951071	8000.158547	13.925440	-0.055945	4.815597
275.893390	8000.198167	13.930445	-0.055934	4.815609
275.556207	8000.115745	13.935450	-0.055871	4.815587
275.651991	8000.156802	13.940455	-0.055889	4.815598
275.640993	8000.159805	13.945459	-0.055886	4.815599
275.341036	8000.115371	13.950464	-0.055830	4.815588
275.472433	8000.183709	13.955469	-0.055854	4.815607
275.685174	8000.155122	13.960474	-0.055894	4.815598
275.637388	8000.182087	13.965479	-0.055885	4.815606
275.456196	8000.157748	13.970483	-0.055851	4.815600
275.732402	8000.148352	13.975488	-0.055902	4.815596
275.804833	8000.154853	13.980493	-0.055915	4.815597
275.493177	8000.114499	13.985498	-0.055857	4.815587
275.692880	8000.173273	13.990503	-0.055894	4.815603
275.625963	8000.194587	13.995507	-0.055881	4.815610
275.549435	8000.139916	14.000512	-0.055867	4.815594
275.512334	8000.138221	14.005517	-0.055859	4.815594
275.381365	8000.121110	14.010522	-0.055835	4.815589
275.487433	8000.165539	14.015527	-0.055854	4.815602
275.403978	8000.121435	14.020531	-0.055838	4.815589
275.394773	8000.143691	14.025536	-0.055837	4.815596
275.693492	8000.123983	14.030541	-0.055892	4.815589
275.536555	8000.131011	14.035546	-0.055862	4.815592
275.605596	8000.155612	14.040551	-0.055875	4.815598
275.741045	8000.143918	14.045555	-0.055900	4.815594
275.827372	8000.125014	14.050560	-0.055916	4.815588
275.778067	8000.181859	14.055565	-0.055906	4.815605
275.902386	8000.116584	14.060570	-0.055929	4.815586
275.975095	8000.186101	14.065575	-0.055943	4.815606
275.757160	8000.172909	14.070579	-0.055902	4.815603
275.767224	8000.153828	14.075584	-0.055903	4.815597
275.745564	8000.186560	14.080589	-0.055899	4.815607
275.705442	8000.142096	14.085594	-0.055891	4.815594
275.621598	8000.209056	14.090599	-0.055876	4.815614
275.822749	8000.146104	14.095603	-0.055913	4.815595
275.660790	8000.143438	14.100608	-0.055882	4.815595
275.598719	8000.112499	14.105613	-0.055871	4.815586
275.661244	8000.097479	14.110618	-0.055882	4.815581
275.721221	8000.144359	14.115623	-0.055893	4.815595
275.585851	8000.149603	14.120627	-0.055867	4.815597
275.539566	8000.129602	14.125632	-0.055859	4.815591
275.763059	8000.195173	14.130637	-0.055900	4.815609
275.718289	8000.138885	14.135642	-0.055891	4.815593
275.723066	8000.170981	14.140647	-0.055892	4.815602
275.650887	8000.153761	14.145651	-0.055878	4.815598
275.835556	8000.136463	14.150656	-0.055912	4.815592
275.734269	8000.254402	14.155661	-0.055893	4.815627
275.719607	8000.181518	14.160666	-0.055890	4.815606
275.879707	8000.147799	14.165671	-0.055920	4.815595
275.749495	8000.131767	14.170675	-0.055895	4.815591
275.610495	8000.133748	14.175680	-0.055869	4.815592
275.750559	8000.173393	14.180685	-0.055895	4.815603
275.510848	8000.154505	14.185690	-0.055850	4.815599
275.610902	8000.150777	14.190695	-0.055869	4.815597
275.619278	8000.142349	14.195699	-0.055870	4.815595
275.743451	8000.133675	14.200704	-0.055893	4.815592
275.799880	8000.123894	14.205709	-0.055903	4.815588
275.683327	8000.104882	14.210714	-0.055881	4.815583
275.824073	8000.144538	14.215719	-0.055907	4.815594
275.882440	8000.134789	14.220723	-0.055918	4.815591
275.792765	8000.138643	14.225728	-0.055901	4.815593
275.669888	8000.160111	14.230733	-0.055878	4.815600
275.733120	8000.175006	14.235738	-0.055889	4.815604
275.632151	8000.172267	14.240743	-0.055870	4.815603
275.765613	8000.189377	14.245747	-0.055895	4.815608
275.757145	8000.158245	14.250752	-0.055893	4.815599
275.806283	8000.195338	14.255757	-0.055902	4.815609
275.623763	8000.101557	14.260762	-0.055868	4.815583
275.925012	8000.144902	14.265767	-0.055923	4.815594
275.677112	8000.122677	14.270771	-0.055877	4.815589
275.753058	8000.135643	14.275776	-0.055891	4.815592
275.789686	8000.191754	14.280781	-0.055898	4.815608
275.590609	8000.120131	14.285786	-0.055860	4.815588
275.596297	7999.165460	14.290791	-0.055860	4.815309

275.534627	7996.026141	14.295795	-0.055847	4.814392
275.501486	7990.596122	14.300800	-0.055837	4.812804
275.540959	7983.963401	14.305805	-0.055839	4.810863
275.477115	7976.617188	14.310810	-0.055822	4.808713
275.591686	7968.999920	14.315815	-0.055839	4.806482
275.591070	7961.216042	14.320819	-0.055833	4.804202
275.376558	7953.405996	14.325824	-0.055788	4.801914
275.471310	7945.395776	14.330829	-0.055800	4.799565
275.308777	7937.435644	14.335834	-0.055764	4.797230
275.341893	7929.378108	14.340839	-0.055765	4.794865
275.324434	7921.429036	14.345843	-0.055756	4.792531
275.255727	7913.338648	14.350848	-0.055738	4.790154
275.309779	7905.497184	14.355853	-0.055743	4.787848
275.231218	7897.332900	14.360858	-0.055723	4.785448
275.300757	7889.408135	14.365863	-0.055730	4.783115
275.180650	7881.407270	14.370867	-0.055702	4.780761
275.103287	7873.402492	14.375872	-0.055682	4.778403
275.299225	7865.434931	14.380877	-0.055713	4.776054
275.277516	7857.382671	14.385882	-0.055704	4.773680
275.267004	7849.417110	14.390887	-0.055697	4.771331
275.470592	7841.374608	14.395891	-0.055729	4.768957
275.419811	7833.424882	14.400896	-0.055714	4.766609
275.266378	7825.379599	14.405901	-0.055680	4.764233
275.335558	7817.407577	14.410906	-0.055687	4.761877
275.312907	7809.362413	14.415911	-0.055678	4.759498
275.207939	7801.437442	14.420915	-0.055653	4.757154
274.884359	7793.351567	14.425920	-0.055587	4.754761
274.897803	7785.315802	14.430925	-0.055584	4.752381
274.787775	7777.279557	14.435930	-0.055558	4.750000
274.969195	7769.328432	14.440935	-0.055586	4.747643
274.936299	7761.328426	14.445939	-0.055575	4.745270
274.737137	7753.324410	14.450944	-0.055532	4.742895
274.798038	7745.345002	14.455949	-0.055538	4.740526
274.893202	7737.359403	14.460954	-0.055550	4.738154
274.852373	7729.335489	14.465959	-0.055537	4.735769
274.795066	7721.356420	14.470963	-0.055521	4.733397
274.671591	7713.292634	14.475968	-0.055493	4.730998
274.728880	7705.319593	14.480973	-0.055498	4.728625
274.798423	7697.281479	14.485978	-0.055505	4.726231
274.736913	7689.335308	14.490983	-0.055489	4.723863
274.495449	7681.321453	14.495987	-0.055438	4.721475
274.438090	7673.312258	14.500992	-0.055422	4.719086
274.713371	7665.408205	14.505997	-0.055468	4.716727
274.452314	7657.288344	14.511002	-0.055414	4.714303
274.528386	7649.293482	14.516007	-0.055422	4.711915
274.741055	7641.283856	14.521011	-0.055457	4.709521
274.500726	7633.312433	14.526016	-0.055406	4.707138
274.278662	7625.324415	14.531021	-0.055360	4.704749
274.162510	7617.308971	14.536026	-0.055332	4.702350
274.238050	7609.286481	14.541031	-0.055341	4.699947
274.003308	7601.343088	14.546035	-0.055292	4.697567
274.153938	7593.281377	14.551040	-0.055314	4.695150
274.240976	7585.304538	14.556045	-0.055325	4.692758
274.006588	7577.267378	14.561050	-0.055276	4.690346
274.200596	7569.252572	14.566055	-0.055307	4.687939
274.254907	7561.284658	14.571059	-0.055311	4.685546
274.069112	7553.316365	14.576064	-0.055271	4.683151
273.898989	7545.301451	14.581069	-0.055234	4.680741
274.063356	7537.282080	14.586074	-0.055259	4.678328
273.843168	7529.327108	14.591079	-0.055213	4.675934
273.965856	7521.247350	14.596083	-0.055230	4.673500
273.991116	7513.098813	14.601088	-0.055229	4.671045
273.816560	7505.228035	14.606093	-0.055192	4.668672
273.663281	7497.206214	14.611098	-0.055157	4.666253
273.673762	7489.253388	14.616103	-0.055154	4.663852
273.608123	7481.207213	14.621107	-0.055136	4.661423
273.624915	7473.262673	14.626112	-0.055134	4.659023
273.480455	7465.295870	14.631117	-0.055102	4.656615
273.594715	7457.198880	14.636122	-0.055117	4.654166
273.598846	7449.226473	14.641127	-0.055113	4.651753
273.378047	7441.191597	14.646131	-0.055066	4.649321
273.332811	7433.236698	14.651136	-0.055052	4.646912
273.380926	7425.220265	14.656141	-0.055056	4.644482
273.358371	7417.244916	14.661146	-0.055046	4.642064
273.392130	7409.205954	14.666151	-0.055047	4.639625
273.465865	7401.264859	14.671155	-0.055055	4.637214
273.308268	7393.204170	14.676160	-0.055020	4.634766
273.140583	7385.211479	14.681165	-0.054984	4.632338
273.062326	7377.140009	14.686170	-0.054964	4.629884
273.137328	7369.218722	14.691175	-0.054972	4.627474
273.154377	7361.185605	14.696179	-0.054970	4.625029
273.051787	7353.202782	14.701184	-0.054945	4.622599
273.076394	7345.188412	14.706189	-0.054944	4.620157
273.012576	7337.205899	14.711194	-0.054927	4.617724
272.976120	7329.152923	14.716199	-0.054915	4.615268
273.127353	7321.180949	14.721203	-0.054938	4.612835
272.935806	7313.164164	14.726208	-0.054896	4.610387
272.983198	7305.182254	14.731213	-0.054900	4.607949
272.942447	7297.136200	14.736218	-0.054887	4.605490
273.014210	7289.159691	14.741223	-0.054895	4.603051
272.833313	7281.191742	14.746227	-0.054856	4.600613
272.751780	7273.172914	14.751232	-0.054835	4.598158
273.004416	7265.174225	14.756237	-0.054876	4.595708
272.776831	7257.102084	14.761242	-0.054829	4.593234
272.653600	7249.110541	14.766247	-0.054800	4.590784
272.674512	7241.134218	14.771251	-0.054799	4.588337
272.680108	7233.117445	14.776256	-0.054794	4.585876
272.500969	7225.156245	14.781261	-0.054755	4.583431
272.385149	7217.128104	14.786266	-0.054728	4.580964
272.689417	7209.168129	14.791271	-0.054780	4.578517
272.462956	7201.164182	14.796275	-0.054732	4.576054
272.343652	7193.113592	14.801280	-0.054704	4.573576
272.418937	7185.126557	14.806285	-0.054713	4.571117
272.598843	7177.121139	14.811290	-0.054741	4.568650
272.343251	7169.116570	14.816295	-0.054688	4.566182
272.355959	7161.111321	14.821299	-0.054685	4.563713
272.551925	7153.135939	14.826304	-0.054716	4.561252
272.327942	7145.157531	14.831309	-0.054669	4.558788
272.215589	7137.156756	14.836314	-0.054642	4.556316
272.338724	7129.113821	14.841319	-0.054660	4.553830
272.318712	7121.108239	14.846323	-0.054650	4.551354
272.283058	7113.087948	14.851328	-0.054638	4.548872
272.322919	7105.101896	14.856333	-0.054640	4.546400
272.262200	7097.079430	14.861338	-0.054624	4.543914
271.984245	7089.117004	14.866343	-0.054566	4.541446
272.031005	7081.120873	14.871347	-0.054570	4.538966
272.051014	7073.118202	14.876352	-0.054568	4.536483
271.942759	7065.121728	14.881357	-0.054542	4.534000
272.015581	7057.082292	14.886362	-0.054550	4.531502
272.015185	7049.070854	14.891367	-0.054545	4.529012
271.979567	7041.130312	14.896371	-0.054533	4.526543
271.740555	7033.089241	14.901376	-0.054483	4.524040
271.869921	7025.167336	14.906381	-0.054501	4.521574
271.767445	7017.114173	14.911386	-0.054477	4.519065
271.577967	7009.165337	14.916391	-0.054436	4.516587
271.724816	7001.091197	14.921395	-0.054458	4.514070
271.681115	6992.982035	14.926400	-0.054444	4.511539
271.811034	6985.006981	14.931405	-0.054463	4.509050
271.438033	6977.051523	14.936410	-0.054388	4.506564
271.583371	6969.012253	14.941415	-0.054410	4.504052
271.593698	6961.103368	14.946419	-0.054406	4.501578
271.400271	6953.040074	14.951424	-0.054365	4.499055
271.430762	6945.118897	14.956429	-0.054365	4.496575
271.314943	6937.023117	14.961434	-0.054338	4.494039
271.564892	6929.036000	14.966439	-0.054379	4.491536
271.484702	6921.030601	14.971443	-0.054359	4.489025
271.395923	6913.038758	14.976448	-0.054337	4.486517
271.398345	6905.060442	14.981453	-0.054332	4.484013
271.178021	6897.076977	14.986458	-0.054285	4.481504
271.367449	6889.075875	14.991463	-0.054315	4.478990
271.293719	6881.058212	14.996467	-0.054296	4.476468
271.162162	6872.998126	15.001472	-0.054266	4.473932
271.248130	6865.012615	15.006477	-0.054276	4.471418
271.098919	6857.003522	15.011482	-0.054243	4.468894
271.070638	6849.017431	15.016487	-0.054232	4.466377
271.083352	6841.077936	15.021491	-0.054229	4.463873
271.159759	6833.009601	15.026496	-0.054238	4.461328
271.183209	6825.078955	15.031501	-0.054237	4.458824
270.790995	6817.021538	15.036506	-0.054158	4.456277
270.857546	6808.999689	15.041511	-0.054165	4.453741
270.627193	6800.999977	15.046515	-0.054117	4.451210
270.754325	6792.967759	15.051520	-0.054135	4.448669
270.896348	6785.000023	15.056525	-0.054156	4.446147
270.596061	6777.040663	15.061530	-0.054095	4.443624
270.644064	6769.026122	15.066535	-0.054098	4.441084
270.635013	6761.047441	15.071539	-0.054091	4.438553
270.481227	6753.013369	15.076544	-0.054057	4.436002
270.595348	6744.978258	15.081549	-0.054073	4.433451
270.455607	6736.898306	15.086554	-0.054041	4.430884
270.414526	6728.954214	15.091559	-0.054028	4.428358
270.514138	6720.962580	15.096563	-0.054041	4.425816
270.335527	6713.000224	15.101568	-0.054003	4.423281
270.344571	6704.978929	15.106573	-0.053999	4.420727
270.371889	6696.983546	15.111578	-0.053998	4.418179
270.137711	6688.976244	15.116583	-0.053949	4.415625
270.263134	6680.990569	15.121587	-0.053967	4.413078
270.203799	6672.917536	15.126592	-0.053951	4.410501
270.157996	6664.989756	15.131597	-0.053937	4.407969
269.960155	6656.952798	15.136602	-0.053894	4.405399
269.941861	6648.980144	15.141607	-0.053886	4.402850
270.141039	6640.985108	15.146611	-0.053917	4.400293
270.041563	6633.010379	15.151616	-0.053893	4.397740
269.931129	6624.978156	15.156621	-0.053867	4.395166
270.007646	6616.953327	15.161626	-0.053876	4.392594
269.966017	6608.941064	15.166631	-0.053863	4.390025
270.063770	6600.994296	15.171635	-0.053876	4.387475
269.957496	6592.963385	15.176640	-0.053850	4.384896
270.070304	6585.026589	15.181645	-0.053866	4.382347
269.941068	6576.984188	15.186650	-0.053836	4.379761
269.824540	6569.016230	15.191655	-0.053809	4.377198
269.848061	6560.998035	15.196659	-0.053808	4.374617
269.675235	6552.962072	15.201664	-0.053770	4.372029
269.792086	6544.955501	15.206669	-0.053787	4.369449
269.650254	6536.986632	15.211674	-0.053755	4.366879
269.750942	6528.934637	15.216679	-0.053768	4.364283
269.587811	6521.040481	15.221683	-0.053732	4.361733
269.601454	6512.985188	15.226688	-0.053729	4.359132
269.662566	6505.012959	15.231693	-0.053735	4.356556
269.408670	6496.920478	15.236698	-0.053683	4.353938
269.371726	6488.849804	15.241703	-0.053670	4.351326
269.566585	6480.861204	15.246707	-0.053701	4.348741
269.435542	6472.885937	15.251712	-0.053671	4.346157
269.360809	6464.922967	15.256717	-0.053652	4.343575
269.325939	6456.940836	15.261722	-0.053640	4.340986
269.206880	6448.970085	15.266727	-0.053612	4.338398
269.244967	6440.989246	15.271731	-0.053614	4.335807
268.946317	6432.921506	15.276736	-0.053553	4.333184
269.174544	6424.882816	15.281741	-0.053590	4.330572
269.227466	6416.922786	15.286746	-0.053594	4.327983
268.952989	6408.909567	15.291751	-0.053538	4.325372
269.034629	6400.955623	15.296755	-0.053547	4.322782
268.863290	6392.936474	15.301760	-0.053510	4.320168
269.080702	6384.993804	15.306765	-0.053545	4.317579
268.974869	6376.941760	15.311770	-0.053520	4.314951
269.128277	6368.909702	15.316775	-0.053543	4.312330
268.965482	6360.882213	15.321779	-0.053507	4.309706
268.840104	6352.897952	15.326784	-0.053478	4.307095
269.056620	6344.934332	15.331789	-0.053513	4.304492
268.838160	6336.912430	15.336794	-0.053467	4.301865
268.736868	6328.925101	15.341799	-0.053443	4.299248
268.964243	6320.935646	15.346803	-0.053480	4.296632
268.971397	6312.907825	15.351808	-0.053476	4.294000
268.872651	6304.934161	15.356813	-0.053452	4.291383
268.681208	6296.903068	15.361818	-0.053411	4.288745
268.796283	6288.887365	15.366823	-0.053427	4.286113
268.679301	6280.899506	15.371827	-0.053399	4.283486
268.529501	6272.916489	15.376832	-0.053366	4.280860
268.717410	6264.960121	15.381837	-0.053396	4.278243
268.537068	6256.915716	15.386842	-0.053356	4.275592
268.343223	6248.859684	15.391847	-0.053315	4.272936
268.424945	6240.822340	15.396851	-0.053325	4.270287
268.472369	6232.868438	15.401856	-0.053328	4.267663
268.522206	6224.846555	15.406861	-0.053332	4.265015
268.407171	6216.908707	15.411866	-0.053305	4.262392
268.362306	6208.885145	15.416871	-0.053291	4.259739
268.432137	6200.914443	15.421875	-0.053299	4.257104
268.197947	6192.873056	15.426880	-0.053250	4.254441
268.327446	6184.868239	15.431885	-0.053268	4.251791
268.395912	6176.875715	15.436890	-0.053276	4.249143
268.116177	6168.897900	15.441895	-0.053218	4.246495
268.179070	6160.858142	15.446899	-0.053224	4.243829
268.102344	6152.873449	15.451904	-0.053204	4.241177
267.955836	6144.923028	15.456909	-0.053172	4.238535
267.832198	6136.905616	15.461914	-0.053143	4.235868
267.997480	6128.879313	15.466919	-0.053169	4.233200
268.050241	6120.890363	15.471923	-0.053173	4.230542
267.881585	6112.897923	15.476928	-0.053136	4.227879
268.078420	6104.876387	15.481933	-0.053167	4.225207
267.980366	6096.944433	15.486938	-0.053144	4.222561
267.534322	6088.914732	15.491943	-0.053055	4.219878
267.721671	6080.946033	15.496947	-0.053085	4.217219
267.706828	6072.900607	15.501952	-0.053076	4.214531
267.663608	6064.893869	15.506957	-0.053063	4.211854
267.541288	6056.874150	15.511962	-0.053034	4.209170
267.486291	6048.923726	15.516967	-0.053019	4.206508
267.639690	6040.954181	15.521971	-0.053042	4.203840
267.477860	6032.927798	15.526976	-0.053006	4.201149
267.693373	6024.958970	15.531981	-0.053041	4.198478
267.478734	6016.930631	15.536986	-0.052996	4.195782
267.312934	6008.826064	15.541991	-0.052959	4.193059
267.393344	6000.819258	15.546995	-0.052969	4.190369
267.229271	5992.834734	15.552000	-0.052933	4.187682
267.393706	5984.855882	15.557005	-0.052958	4.185000
267.367113	5976.896666	15.562010	-0.052947	4.182320
267.132279	5968.837309	15.567015	-0.052898	4.179602
267.246220	5960.913431	15.572019	-0.052914	4.176932
267.194000	5952.888148	15.577024	-0.052899	4.174224
267.170831	5944.901343	15.582029	-0.052889	4.171528
266.984487	5936.857748	15.587034	-0.052849	4.168809
266.899238	5928.867780	15.592039	-0.052828	4.166108
267.033959	5920.890325	15.597043	-0.052847	4.163411
267.100948	5912.848375	15.602048	-0.052854	4.160691
266.989219	5904.916422	15.607053	-0.052828	4.158003
266.884758	5896.899140	15.612058	-0.052803	4.155285
266.862092	5888.828167	15.617063	-0.052793	4.152548
267.016477	5880.853841	15.622067	-0.052817	4.149844
266.887225	5872.838558	15.627072	-0.052787	4.147121
266.798232	5864.855653	15.632077	-0.052765	4.144408
266.886562	5856.921290	15.637082	-0.052776	4.141711
266.834028	5848.865913	15.642087	-0.052761	4.138970
266.683533	5840.901931	15.647091	-0.052727	4.136257
266.481298	5832.862658	15.652096	-0.052684	4.133516
266.712294	5824.834135	15.657101	-0.052722	4.130782
266.640114	5816.830142	15.662106	-0.052703	4.128051
266.692744	5808.856163	15.667111	-0.052707	4.125330
266.746436	5800.930339	15.672115	-0.052712	4.122623
266.471766	5792.860257	15.677120	-0.052655	4.119862
266.266774	5784.957365	15.682125	-0.052612	4.117156
266.357826	5776.881784	15.687130	-0.052623	4.114393
266.240227	5768.823103	15.692135	-0.052596	4.111632
266.205716	5760.857815	15.697139	-0.052584	4.108902
266.067067	5752.825359	15.702144	-0.052552	4.106145
266.135832	5744.852273	15.707149	-0.052560	4.103410
265.927937	5736.880577	15.712154	-0.052516	4.100670
266.174925	5728.871296	15.717159	-0.052556	4.097921
266.281440	5720.860951	15.722163	-0.052571	4.095168
265.910579	5712.855538	15.727168	-0.052496	4.092409
265.844866	5704.845532	15.732173	-0.052478	4.089650
265.912383	5696.884629	15.737178	-0.052485	4.086908
266.057222	5688.868054	15.742183	-0.052507	4.084146
265.971235	5680.939307	15.747187	-0.052486	4.081409
265.951464	5672.872255	15.752192	-0.052476	4.078623
265.931160	5664.920056	15.757197	-0.052467	4.075876
265.878911	5656.910431	15.762202	-0.052452	4.073106
265.842704	5648.868647	15.767207	-0.052440	4.070323
265.907287	5640.907609	15.772211	-0.052446	4.067568
265.698072	5632.886584	15.777216	-0.052402	4.064786
265.750800	5624.936888	15.782221	-0.052406	4.062031
265.589059	5616.944761	15.787226	-0.052371	4.059256
265.611347	5608.927154	15.792231	-0.052369	4.056473
265.587900	5600.877427	15.797235	-0.052360	4.053677
265.724612	5592.862469	15.802240	-0.052380	4.050892
265.804954	5584.919945	15.807245	-0.052389	4.048131
265.611198	5576.920893	15.812250	-0.052348	4.045343
265.532401	5568.928829	15.817255	-0.052327	4.042558
265.467733	5560.912164	15.822259	-0.052310	4.039763
265.338055	5552.951290	15.827264	-0.052280	4.036984
265.462337	5544.872364	15.832269	-0.052298	4.034166
265.160492	5536.796933	15.837274	-0.052236	4.031340
265.138972	5528.840106	15.842279	-0.052227	4.028559
264.981906	5520.859914	15.847283	-0.052192	4.025765
265.087570	5512.890751	15.852288	-0.052206	4.022977
265.279612	5504.906343	15.857293	-0.052237	4.020183
265.000608	5496.921545	15.862298	-0.052179	4.017380
265.018327	5488.854523	15.867303	-0.052177	4.014550
265.221667	5480.845360	15.872307	-0.052209	4.011742
264.919535	5472.851950	15.877312	-0.052148	4.008929
264.858867	5464.904907	15.882317	-0.052131	4.006135
264.969956	5456.920187	15.887322	-0.052146	4.003328
264.799068	5448.884679	15.892327	-0.052109	4.000496
264.819290	5440.933048	15.897331	-0.052107	3.997696
264.619907	5432.902315	15.902336	-0.052065	3.994862
264.889004	5424.848749	15.907341	-0.052109	3.992025
264.778514	5416.869610	15.912346	-0.052083	3.989206
264.822516	5408.860729	15.917351	-0.052086	3.986378
264.639906	5400.895442	15.922355	-0.052047	3.983559
264.536984	5392.880101	15.927360	-0.052022	3.980722
264.714520	5384.930526	15.932365	-0.052050	3.977910
264.770864	5376.905887	15.937370	-0.052055	3.975068
264.540680	5368.865323	15.942375	-0.052006	3.972214
264.595077	5360.865498	15.947379	-0.052011	3.969377
264.419941	5352.883212	15.952384	-0.051973	3.966540
264.483620	5344.940950	15.957389	-0.051979	3.963719
264.350143	5336.957631	15.962394	-0.051949	3.960878
264.060783	5328.990266	15.967399	-0.051890	3.958039
264.246140	5320.946996	15.972403	-0.051919	3.955178
264.310186	5312.884726	15.977408	-0.051925	3.952306
264.390920	5304.882621	15.982413	-0.051935	3.949454
264.222710	5296.935222	15.987418	-0.051898	3.946615
264.142539	5288.916742	15.992423	-0.051877	3.943751
264.199589	5280.967208	15.997427	-0.051883	3.940911
264.232401	5272.973974	16.002432	-0.051883	3.938053
264.274293	5264.938992	16.007437	-0.051886	3.935178
264.210564	5256.916029	16.012442	-0.051868	3.932304
263.974707	5248.931998	16.017447	-0.051819	3.929438
263.997611	5240.985224	16.022451	-0.051818	3.926588
263.867787	5232.931088	16.027456	-0.051788	3.923695
263.875483	5224.988050	16.032461	-0.051784	3.920842
263.801166	5216.981180	16.037466	-0.051765	3.917963
264.061680	5208.962222	16.042471	-0.051808	3.915083
264.009649	5200.965127	16.047475	-0.051793	3.912203
263.768579	5192.936056	16.052480	-0.051742	3.909307
263.849440	5184.987269	16.057485	-0.051752	3.906442
263.857626	5176.941663	16.062490	-0.051748	3.903540
263.616704	5168.937517	16.067495	-0.051698	3.900645
263.781451	5160.974321	16.072499	-0.051723	3.897771
263.796822	5152.964369	16.077504	-0.051720	3.894875
263.552020	5144.953404	16.082509	-0.051669	3.891972
263.529905	5136.927256	16.087514	-0.051660	3.889065
263.735659	5128.939797	16.092519	-0.051693	3.886174
263.760107	5120.963568	16.097523	-0.051692	3.883282
263.549404	5112.948255	16.102528	-0.051647	3.880369
263.499277	5105.013777	16.107533	-0.051632	3.877486
263.627136	5096.968307	16.112538	-0.051650	3.874564
263.314219	5088.695330	16.117543	-0.051587	3.871549
263.551496	5080.818267	16.122547	-0.051625	3.868686
263.378756	5072.869916	16.127552	-0.051588	3.865787
263.231655	5064.916791	16.132557	-0.051555	3.862884
263.240109	5056.921828	16.137562	-0.051551	3.859967
263.148778	5048.955504	16.142567	-0.051529	3.857057
263.330894	5040.977562	16.147571	-0.051557	3.854145
263.221136	5032.909117	16.152576	-0.051531	3.851192
263.204424	5024.956005	16.157581	-0.051523	3.848281
263.228916	5016.959758	16.162586	-0.051522	3.845353
263.096550	5008.980944	16.167591	-0.051492	3.842426
262.988004	5001.015443	16.172595	-0.051466	3.839502
263.074685	4993.005939	16.177600	-0.051477	3.836564
263.032002	4984.987779	16.182605	-0.051463	3.833617
262.954037	4976.982908	16.187610	-0.051443	3.830672
262.904822	4968.967327	16.192615	-0.051429	3.827722
262.953755	4961.001496	16.197619	-0.051432	3.824790
262.574407	4953.025693	16.202624	-0.051356	3.821843
262.632721	4945.036929	16.207629	-0.051362	3.818898
262.727002	4937.056460	16.212634	-0.051374	3.815954
262.586356	4929.033212	16.217639	-0.051342	3.812988
262.566683	4921.020213	16.222643	-0.051333	3.810025
262.621848	4913.047900	16.227648	-0.051338	3.807077
262.523056	4905.042714	16.232653	-0.051314	3.804111
262.376412	4897.078639	16.237658	-0.051281	3.801157
262.370292	4889.056154	16.242663	-0.051275	3.798182
262.437009	4881.061725	16.247667	-0.051282	3.795217
262.475835	4873.004593	16.252672	-0.051283	3.792225
262.455463	4864.996796	16.257677	-0.051274	3.789249
262.325941	4857.043774	16.262682	-0.051244	3.786287
262.365277	4849.020694	16.267687	-0.051246	3.783302
262.194789	4841.080211	16.272691	-0.051209	3.780339
262.230248	4833.094275	16.277696	-0.051210	3.777363
262.139835	4825.045298	16.282701	-0.051188	3.774357
261.878034	4817.070841	16.287706	-0.051134	3.771373
261.742453	4809.030003	16.292711	-0.051103	3.768365
262.045747	4801.056450	16.297715	-0.051154	3.765389
261.771129	4793.068629	16.302720	-0.051097	3.762393
261.688558	4785.069663	16.307725	-0.051077	3.759394
261.804261	4777.121496	16.312730	-0.051093	3.756416
261.742477	4769.066646	16.317735	-0.051076	3.753392
261.581480	4761.056886	16.322739	-0.051040	3.750381
261.489825	4753.063437	16.327744	-0.051018	3.747374
261.692191	4745.040671	16.332749	-0.051050	3.744361
261.591457	4737.103779	16.337754	-0.051026	3.741371
261.477926	4729.065577	16.342759	-0.050999	3.738340
261.620082	4721.112192	16.347763	-0.051020	3.735344
261.468459	4713.096040	16.352768	-0.050987	3.732316
261.568735	4705.057277	16.357773	-0.051000	3.729282
261.646552	4697.094974	16.362778	-0.051009	3.726274
261.619746	4689.121821	16.367783	-0.050998	3.723257
261.451200	4681.135367	16.372787	-0.050961	3.720230
261.362669	4673.170128	16.377792	-0.050940	3.717209
261.424801	4665.130937	16.382797	-0.050946	3.714162
261.356383	4657.010546	16.387802	-0.050927	3.711079
261.197760	4649.026019	16.392807	-0.050892	3.708042
261.266729	4641.091614	16.397811	-0.050900	3.705027
261.278043	4633.125567	16.402816	-0.050896	3.701997
261.278367	4625.140535	16.407821	-0.050891	3.698956
261.201736	4617.188410	16.412826	-0.050871	3.695924
261.272814	4609.138230	16.417831	-0.050879	3.692855
261.296228	4601.135466	16.422835	-0.050878	3.689801
261.151561	4593.183110	16.427840	-0.050846	3.686759
261.070094	4585.205446	16.432845	-0.050825	3.683707
261.058244	4577.195558	16.437850	-0.050817	3.680641
260.938369	4569.210965	16.442855	-0.050790	3.677580
260.773794	4561.197806	16.447859	-0.050753	3.674504
260.717498	4553.169531	16.452864	-0.050738	3.671423
260.698865	4545.181256	16.457869	-0.050729	3.668355
260.696464	4537.181529	16.462874	-0.050723	3.665281
260.630027	4529.198534	16.467879	-0.050705	3.662209
260.637188	4521.221334	16.472883	-0.050701	3.659139
260.553370	4513.204370	16.477888	-0.050680	3.656048
260.762948	4505.164498	16.482893	-0.050713	3.652953
260.834574	4497.167479	16.487898	-0.050721	3.649869
260.677824	4489.201752	16.492903	-0.050686	3.646788
260.807028	4481.213468	16.497907	-0.050705	3.643704
260.680028	4473.228605	16.502912	-0.050676	3.640611
260.469397	4465.267659	16.507917	-0.050631	3.637523
260.506512	4457.227939	16.512922	-0.050633	3.634408
260.477424	4449.180399	16.517927	-0.050622	3.631286
260.543883	4441.199852	16.522931	-0.050629	3.628189
260.409249	4433.187960	16.527936	-0.050598	3.625073
260.412669	4425.223894	16.532941	-0.050593	3.621975
260.315280	4417.229639	16.537946	-0.050570	3.618861
260.070043	4409.238328	16.542951	-0.050519	3.615741
260.340692	4401.257553	16.547955	-0.050564	3.612637
260.115144	4393.232354	16.552960	-0.050516	3.609499
259.992902	4385.287593	16.557965	-0.050488	3.606393
259.938049	4377.318587	16.562970	-0.050472	3.603276
259.907403	4369.282192	16.567975	-0.050461	3.600131
260.016645	4361.353581	16.572979	-0.050476	3.597029
259.940867	4353.300155	16.577984	-0.050456	3.593871
259.993715	4345.285944	16.582989	-0.050461	3.590729
259.929662	4337.333282	16.587994	-0.050444	3.587604
259.777497	4329.322496	16.592999	-0.050410	3.584452
259.957645	4321.367677	16.598003	-0.050438	3.581329
259.846092	4313.348229	16.603008	-0.050412	3.578168
259.659658	4305.360401	16.608013	-0.050371	3.575016
259.731113	4297.367149	16.613018	-0.050379	3.571866
259.618527	4289.343048	16.618023	-0.050353	3.568695
259.553173	4281.365314	16.623027	-0.050335	3.565542
259.509933	4273.371730	16.628032	-0.050322	3.562380
259.576702	4265.385011	16.633037	-0.050329	3.559221
259.839493	4257.411293	16.638042	-0.050372	3.556070
259.563602	4249.308300	16.643047	-0.050315	3.552850
259.456844	4241.281166	16.648051	-0.050290	3.549661
259.591355	4233.318680	16.653056	-0.050310	3.546503
259.343785	4225.350281	16.658061	-0.050258	3.543328
259.337000	4217.382803	16.663066	-0.050251	3.540157
259.264167	4209.385921	16.668071	-0.050232	3.536970
259.351055	4201.392042	16.673075	-0.050243	3.533786
259.133811	4193.397092	16.678080	-0.050197	3.530590
259.042046	4185.397610	16.683085	-0.050175	3.527393
259.089267	4177.389379	16.688090	-0.050178	3.524193
258.883633	4169.438133	16.693095	-0.050134	3.521006
258.900789	4161.456869	16.698099	-0.050132	3.517811
258.979103	4153.427552	16.703104	-0.050141	3.514595
258.946377	4145.438990	16.708109	-0.050129	3.511389
258.886462	4137.434192	16.713114	-0.050113	3.508173
258.897293	4129.411111	16.718119	-0.050109	3.504949
258.963466	4121.497402	16.723123	-0.050116	3.501768
258.866053	4113.487313	16.728128	-0.050093	3.498540
258.862368	4105.495177	16.733133	-0.050087	3.495319
258.859524	4097.501840	16.738138	-0.050081	3.492095
258.738138	4089.484981	16.743143	-0.050052	3.488854
258.580389	4081.520184	16.748147	-0.050018	3.485630
258.611235	4073.534882	16.753152	-0.050018	3.482401
258.678446	4065.534071	16.758157	-0.050025	3.479164
258.372505	4057.573262	16.763162	-0.049963	3.475928
258.468035	4049.498187	16.768167	-0.049975	3.472655
258.498043	4041.512749	16.773171	-0.049975	3.469414
258.431493	4033.524794	16.778176	-0.049957	3.466166
258.409825	4025.543082	16.783181	-0.049948	3.462918
258.379565	4017.553466	16.788186	-0.049937	3.459664
258.096544	4009.586303	16.793191	-0.049878	3.456408
258.131720	4001.591253	16.798195	-0.049880	3.453148
258.107330	3993.556576	16.803200	-0.049870	3.449866
258.132933	3985.579731	16.808205	-0.049869	3.446607
258.004971	3977.599979	16.813210	-0.049840	3.443338
257.887877	3969.621652	16.818215	-0.049812	3.440067
258.046186	3961.633892	16.823219	-0.049836	3.436798
257.892629	3953.616731	16.828224	-0.049802	3.433504
258.120101	3945.569349	16.833229	-0.049839	3.430207
258.180966	3937.600196	16.838234	-0.049845	3.426933
258.093655	3929.600750	16.843239	-0.049823	3.423639
258.039405	3921.654063	16.848243	-0.049808	3.420364
258.109760	3913.653259	16.853248	-0.049815	3.417068
257.984325	3905.647608	16.858253	-0.049787	3.413760
257.983823	3897.659063	16.863258	-0.049781	3.410461
257.779782	3889.664227	16.868263	-0.049738	3.407148
257.787810	3881.693530	16.873267	-0.049734	3.403850
257.853610	3873.699372	16.878272	-0.049740	3.400541
257.818027	3865.733497	16.883277	-0.049728	3.397236
257.784363	3857.736138	16.888282	-0.049717	3.393916
257.696235	3849.633287	16.893287	-0.049695	3.390546
257.428982	3841.711953	16.898291	-0.049640	3.387242
257.469429	3833.708022	16.903296	-0.049642	3.383912
257.533736	3825.736147	16.908301	-0.049648	3.380592
257.439363	3817.793023	16.913306	-0.049625	3.377276
257.109000	3809.788883	16.918311	-0.049558	3.373922
257.614451	3801.737297	16.923315	-0.049647	3.370575
257.426272	3793.784062	16.928320	-0.049606	3.367241
257.261982	3785.786827	16.933325	-0.049570	3.363886
257.350798	3777.810919	16.938330	-0.049581	3.360546
257.216909	3769.818182	16.943335	-0.049551	3.357187
257.209243	3761.833033	16.948339	-0.049544	3.353833
256.937885	3753.804446	16.953344	-0.049488	3.350447
256.948792	3745.812307	16.958349	-0.049485	3.347084
256.987871	3737.825015	16.963354	-0.049487	3.343720
256.822539	3729.841329	16.968359	-0.049450	3.340347
256.965803	3721.878066	16.973363	-0.049472	3.336991
256.870181	3713.872732	16.978368	-0.049448	3.333605
256.832639	3705.830664	16.983373	-0.049436	3.330201
256.996630	3697.851373	16.988378	-0.049461	3.326829
256.793049	3689.882244	16.993383	-0.049418	3.323443
256.907594	3681.905800	16.998387	-0.049433	3.320063
256.664676	3673.970473	17.003392	-0.049383	3.316683
256.759007	3665.915890	17.008397	-0.049395	3.313262
256.842429	3657.879351	17.013402	-0.049405	3.309845
256.587284	3649.919264	17.018407	-0.049352	3.306444
256.620823	3641.957868	17.023411	-0.049353	3.303049
256.637447	3633.979111	17.028416	-0.049350	3.299644
256.538645	3626.006506	17.033421	-0.049327	3.296233
256.726898	3617.974159	17.038426	-0.049356	3.292803
256.501922	3609.950073	17.043431	-0.049309	3.289358
256.315717	3602.024179	17.048435	-0.049269	3.285953
256.087067	3594.061711	17.053440	-0.049221	3.282527
256.286099	3586.026131	17.058445	-0.049252	3.279082
256.356681	3578.057709	17.063450	-0.049260	3.275658
256.085957	3570.027847	17.068455	-0.049204	3.272191
256.119458	3562.032515	17.073459	-0.049205	3.268746
256.143268	3554.036358	17.078464	-0.049204	3.265297
256.037861	3546.087187	17.083469	-0.049179	3.261860
256.007854	3538.107787	17.088474	-0.049168	3.258409
256.032331	3530.100856	17.093479	-0.049167	3.254944
256.032227	3522.103264	17.098483	-0.049161	3.251479
256.011406	3514.096687	17.103488	-0.049152	3.248006
255.917700	3506.105423	17.108493	-0.049129	3.244532
256.098752	3498.161940	17.113498	-0.049157	3.241087
255.874727	3490.165437	17.118503	-0.049110	3.237598
255.847897	3482.161483	17.123507	-0.049100	3.234111
255.673001	3474.125591	17.128512	-0.049062	3.230599
255.664301	3466.121608	17.133517	-0.049055	3.227105
255.793725	3458.145514	17.138522	-0.049073	3.223624
255.725875	3450.162231	17.143527	-0.049055	3.220129
255.859440	3442.200796	17.148531	-0.049075	3.216648
255.722219	3434.209354	17.153536	-0.049044	3.213138
255.554115	3426.194081	17.158541	-0.049007	3.209613
255.716455	3418.237425	17.163546	-0.049032	3.206124
255.379531	3410.281308	17.168551	-0.048963	3.202610
255.553953	3402.278481	17.173555	-0.048991	3.199093
255.481589	3394.297224	17.178560	-0.048972	3.195571
255.301869	3386.284836	17.183565	-0.048933	3.192028
255.367180	3378.280642	17.188570	-0.048939	3.188494
255.420472	3370.274452	17.193575	-0.048944	3.184955
255.243482	3362.342901	17.198579	-0.048905	3.181435
255.165114	3354.348102	17.203584	-0.048885	3.177887
255.295952	3346.312609	17.208589	-0.048904	3.174327
255.209866	3338.359662	17.213594	-0.048883	3.170790
255.085824	3330.360378	17.218599	-0.048854	3.167226
255.219040	3322.378886	17.223603	-0.048874	3.163678
255.125393	3314.415698	17.228608	-0.048851	3.160124
254.760910	3306.459184	17.233613	-0.048777	3.156557
254.787768	3298.460460	17.238618	-0.048777	3.152984
254.752472	3290.412686	17.243623	-0.048765	3.149382
254.943748	3282.422352	17.248627	-0.048795	3.145812
254.908059	3274.434702	17.253632	-0.048783	3.142229
254.708323	3266.467425	17.258637	-0.048740	3.138644
254.787666	3258.495786	17.263642	-0.048750	3.135066
254.660135	3250.482862	17.268647	-0.048720	3.131455
254.645632	3242.520041	17.273651	-0.048712	3.127868
254.789071	3234.491920	17.278656	-0.048734	3.124254
254.619887	3226.553086	17.283661	-0.048697	3.120663
254.536290	3218.585293	17.288666	-0.048676	3.117058
254.465969	3210.581998	17.293671	-0.048657	3.113433
254.446224	3202.574754	17.298675	-0.048648	3.109805
254.380333	3194.578039	17.303680	-0.048630	3.106175
254.425138	3186.594056	17.308685	-0.048633	3.102551
254.448568	3178.631821	17.313690	-0.048632	3.098933
254.092353	3170.656017	17.318695	-0.048560	3.095286
254.205915	3162.660982	17.323699	-0.048576	3.091648
254.418976	3154.659110	17.328704	-0.048610	3.088007
254.089181	3146.664743	17.333709	-0.048543	3.084340
253.887173	3138.755127	17.338714	-0.048500	3.080714
254.023776	3130.734025	17.343719	-0.048520	3.077048
254.157022	3122.698935	17.348723	-0.048540	3.073371
253.991575	3114.658268	17.353728	-0.048503	3.069673
253.839943	3106.697266	17.358733	-0.048470	3.066007
253.823521	3098.751030	17.363738	-0.048461	3.062351
253.548385	3090.768990	17.368743	-0.048404	3.058661
253.524861	3082.808793	17.373747	-0.048395	3.054989
253.582247	3074.785666	17.378752	-0.048400	3.051287
253.704481	3066.783117	17.383757	-0.048417	3.047594
253.622603	3058.810600	17.388762	-0.048396	3.043900
253.496688	3050.859765	17.393767	-0.048368	3.040209
253.466971	3042.917430	17.398771	-0.048357	3.036523
253.489449	3034.882620	17.403776	-0.048355	3.032791
253.623508	3026.854811	17.408781	-0.048375	3.029064
253.681704	3018.884919	17.413786	-0.048380	3.025355
253.547891	3010.930087	17.418791	-0.048350	3.021640
253.321329	3002.977430	17.423795	-0.048302	3.017916
253.248187	2994.986597	17.428800	-0.048283	3.014178
253.303624	2986.951557	17.433805	-0.048288	3.010420
253.258942	2978.995644	17.438810	-0.048274	3.006690
253.247182	2970.997615	17.443815	-0.048267	3.002937
253.471118	2963.009964	17.448819	-0.048303	2.999196
253.235068	2955.073492	17.453824	-0.048253	2.995451
253.092433	2947.057008	17.458829	-0.048221	2.991669
253.261302	2939.046143	17.463834	-0.048247	2.987900
253.121733	2931.059579	17.468839	-0.048216	2.984123
253.100116	2923.093084	17.473843	-0.048207	2.980356
253.042859	2915.137181	17.478848	-0.048190	2.976587
253.126368	2907.128282	17.483853	-0.048200	2.972796
253.055035	2899.159286	17.488858	-0.048182	2.969010
252.791136	2891.192908	17.493863	-0.048127	2.965212
252.838665	2883.231618	17.498867	-0.048131	2.961427
252.600915	2875.256825	17.503872	-0.048081	2.957616
252.568680	2867.232993	17.508877	-0.048069	2.953787
252.665306	2859.233754	17.513882	-0.048082	2.949972
252.462829	2851.263481	17.518887	-0.048039	2.946150
252.472379	2843.292403	17.523891	-0.048035	2.942333
252.451805	2835.319967	17.528896	-0.048026	2.938510
252.526931	2827.303316	17.533901	-0.048034	2.934665
252.478671	2819.344331	17.538906	-0.048020	2.930836
252.164884	2811.349573	17.543911	-0.047956	2.926972
252.226060	2803.381496	17.548915	-0.047962	2.923135
252.349068	2795.404793	17.553920	-0.047979	2.919291
251.954569	2787.461113	17.558925	-0.047901	2.915432
252.144085	2779.374974	17.563930	-0.047930	2.911529
252.110007	2771.383443	17.568935	-0.047919	2.907655
252.073927	2763.409877	17.573939	-0.047906	2.903784
251.964146	2755.467953	17.578944	-0.047881	2.899920
252.047191	2747.494161	17.583949	-0.047891	2.896045
252.102122	2739.498890	17.588954	-0.047895	2.892153
251.784128	2731.523809	17.593959	-0.047831	2.888246
251.992097	2723.517120	17.598963	-0.047864	2.884346
252.027267	2715.591444	17.603968	-0.047865	2.880471
251.583414	2707.631816	17.608973	-0.047777	2.876548
251.688648	2699.635849	17.613978	-0.047791	2.872632
251.640232	2691.616494	17.618983	-0.047777	2.868691
251.537810	2683.645335	17.623987	-0.047752	2.864765
251.509679	2675.691374	17.628992	-0.047741	2.860846
251.519647	2667.697853	17.633997	-0.047738	2.856905
251.647898	2659.720333	17.639002	-0.047756	2.852972
251.350892	2651.729260	17.644007	-0.047696	2.849004
251.529976	2643.741566	17.649011	-0.047723	2.845059
251.506924	2635.811062	17.654016	-0.047714	2.841124
251.373601	2627.828691	17.659021	-0.047683	2.837153
251.358634	2619.848493	17.664026	-0.047675	2.833184
251.422752	2611.803436	17.669031	-0.047682	2.829181
251.280814	2603.849565	17.674035	-0.047650	2.825206
251.079429	2595.904394	17.679040	-0.047607	2.821227
251.224247	2587.916526	17.684045	-0.047628	2.817241
251.311898	2579.921529	17.689050	-0.047639	2.813242
250.864513	2571.960795	17.694055	-0.047551	2.809223
250.948356	2563.968536	17.699059	-0.047561	2.805214
251.043098	2555.998805	17.704064	-0.047573	2.801211
250.868845	2548.033712	17.709069	-0.047535	2.797189
250.820029	2540.068747	17.714074	-0.047520	2.793168
250.720963	2532.059341	17.719079	-0.047497	2.789117
250.577372	2524.098868	17.724083	-0.047464	2.785081
250.580922	2516.135360	17.729088	-0.047460	2.781047
250.817554	2508.120584	17.734093	-0.047498	2.776994
250.827818	2500.147477	17.739098	-0.047495	2.772944
250.595246	2492.160446	17.744103	-0.047446	2.768866
250.440971	2484.213487	17.749107	-0.047412	2.764807
250.680816	2476.231451	17.754112	-0.047451	2.760748
250.537844	2468.266314	17.759117	-0.047419	2.756668
250.519809	2460.272138	17.764122	-0.047410	2.752575
250.393517	2452.234459	17.769127	-0.047381	2.748448
250.287059	2444.278897	17.774131	-0.047356	2.744357
250.263917	2436.336325	17.779136	-0.047346	2.740272
250.179928	2428.375860	17.784141	-0.047325	2.736167
250.117363	2420.401855	17.789146	-0.047308	2.732051
250.079993	2412.385565	17.794151	-0.047296	2.727909
249.987462	2404.447745	17.799155	-0.047273	2.723797
249.911608	2396.490466	17.804160	-0.047253	2.719670
250.055893	2388.505193	17.809165	-0.047275	2.715536
250.005716	2380.517431	17.814170	-0.047260	2.711382
249.924625	2372.537248	17.819175	-0.047239	2.707224
249.731751	2364.592956	17.824179	-0.047198	2.703071
249.671623	2356.626504	17.829184	-0.047181	2.698909
249.762829	2348.618957	17.834189	-0.047193	2.694728
249.795205	2340.638025	17.839194	-0.047194	2.690550
249.550899	2332.680273	17.844199	-0.047143	2.686361
249.451844	2324.727601	17.849203	-0.047119	2.682177
249.633323	2316.744517	17.854208	-0.047147	2.677989
249.562006	2308.755941	17.859213	-0.047128	2.673775
249.470436	2300.768273	17.864218	-0.047106	2.669553
249.472182	2292.773672	17.869223	-0.047101	2.665327
249.357941	2284.848309	17.874227	-0.047074	2.661124
249.221620	2276.891754	17.879232	-0.047043	2.656896
249.034215	2268.911901	17.884237	-0.047003	2.652645
249.055479	2260.931994	17.889242	-0.047001	2.648401
249.236854	2252.926194	17.894247	-0.047030	2.644147
249.236528	2244.984721	17.899251	-0.047024	2.639909
249.313860	2237.011428	17.904256	-0.047033	2.635652
249.094081	2229.014471	17.909261	-0.046987	2.631355
248.826082	2221.096857	17.914266	-0.046931	2.627091
248.958768	2213.079412	17.919271	-0.046951	2.622793
249.243425	2205.101142	17.924275	-0.046998	2.618519
248.885863	2197.180938	17.929280	-0.046926	2.614227
248.728070	2189.198862	17.934285	-0.046891	2.609907
248.752357	2181.238591	17.939290	-0.046891	2.605604
248.915314	2173.247967	17.944295	-0.046915	2.601288
248.827452	2165.300946	17.949299	-0.046894	2.596970
248.675346	2157.228270	17.954304	-0.046860	2.592573
248.664334	2149.166327	17.959309	-0.046852	2.588183
248.438030	2141.267194	17.964314	-0.046805	2.583861
248.226863	2133.332107	17.969319	-0.046760	2.579512
248.421556	2125.360907	17.974323	-0.046791	2.575164
248.445102	2117.402978	17.979328	-0.046790	2.570804
248.348995	2109.431575	17.984333	-0.046766	2.566422
248.627588	2101.464227	17.989338	-0.046813	2.562060
248.367504	2093.537945	17.994343	-0.046759	2.557675
248.126643	2085.591314	17.999347	-0.046709	2.553273
248.134507	2077.592821	18.004352	-0.046705	2.548853
248.122922	2069.604470	18.009357	-0.046697	2.544428
248.085319	2061.692094	18.014362	-0.046685	2.540037
247.895788	2053.728301	18.019367	-0.046644	2.535598
247.985355	2045.732561	18.024371	-0.046655	2.531154
248.062234	2037.768929	18.029376	-0.046664	2.526719
248.047403	2029.802214	18.034381	-0.046656	2.522268
248.087214	2021.867923	18.039386	-0.046658	2.517831
247.839672	2013.891293	18.044391	-0.046606	2.513341
247.632688	2005.914124	18.049395	-0.046562	2.508847
247.615309	1997.934430	18.054400	-0.046554	2.504356
247.644057	1989.972233	18.059405	-0.046554	2.499871
247.579465	1982.038575	18.064410	-0.046536	2.495387
247.640297	1974.026603	18.069415	-0.046542	2.490859
247.442189	1966.080604	18.074419	-0.046500	2.486342
247.344332	1958.144942	18.079424	-0.046476	2.481830
247.125353	1950.211266	18.084429	-0.046430	2.477301
247.358493	1942.206269	18.089434	-0.046468	2.472758
247.276024	1934.208076	18.094439	-0.046447	2.468186
247.042610	1926.274455	18.099443	-0.046398	2.463631
247.179040	1918.310277	18.104448	-0.046418	2.459079
247.132945	1910.361292	18.109453	-0.046404	2.454512
247.241754	1902.376976	18.114458	-0.046419	2.449929
247.188098	1894.410187	18.119463	-0.046403	2.445335
247.109004	1886.488220	18.124467	-0.046383	2.440756
246.993198	1878.546088	18.129472	-0.046356	2.436154
246.736845	1870.526947	18.134477	-0.046303	2.431488
246.869191	1862.524389	18.139482	-0.046322	2.426852
246.916978	1854.571813	18.144487	-0.046326	2.422230
246.706603	1846.650117	18.149491	-0.046281	2.417597
246.511436	1838.717142	18.154496	-0.046239	2.412950
246.584879	1830.702295	18.159501	-0.046248	2.408267
246.472500	1822.776665	18.164506	-0.046221	2.403613
246.287938	1814.845002	18.169511	-0.046182	2.398940
246.490901	1806.854130	18.174515	-0.046214	2.394254
246.500905	1798.865406	18.179520	-0.046210	2.389544
246.256134	1790.935490	18.184525	-0.046159	2.384840
246.250232	1783.000156	18.189530	-0.046153	2.380143
246.360622	1775.013340	18.194535	-0.046168	2.375414
246.199230	1767.056310	18.199539	-0.046132	2.370673
246.160001	1759.106971	18.204544	-0.046120	2.365936
246.284881	1751.141776	18.209549	-0.046137	2.361193
246.155500	1743.238032	18.214554	-0.046108	2.356457
245.861393	1735.257208	18.219559	-0.046048	2.351652
245.872207	1727.284071	18.224563	-0.046044	2.346866
245.902543	1719.317275	18.229568	-0.046045	2.342077
245.823440	1711.367635	18.234573	-0.046024	2.337278
245.899604	1703.413770	18.239578	-0.046033	2.332480
245.783518	1695.446992	18.244583	-0.046006	2.327649
245.724672	1687.503416	18.249587	-0.045990	2.322826
245.697685	1679.574326	18.254592	-0.045979	2.318004
245.640534	1671.610562	18.259597	-0.045963	2.313149
245.741695	1663.632929	18.264602	-0.045977	2.308288
245.422307	1655.704185	18.269607	-0.045912	2.303412
245.466437	1647.748375	18.274611	-0.045914	2.298539
245.658287	1639.788831	18.279616	-0.045945	2.293667
245.421967	1631.832053	18.284621	-0.045895	2.288749
245.334726	1623.902305	18.289626	-0.045874	2.283850
245.457984	1615.936594	18.294631	-0.045891	2.278936
245.374127	1607.997977	18.299635	-0.045870	2.274010
245.305085	1599.973594	18.304640	-0.045852	2.269022
245.339380	1592.005940	18.309645	-0.045853	2.264067
245.432495	1584.081532	18.314650	-0.045865	2.259134
245.068308	1576.182798	18.319655	-0.045791	2.254165
244.960840	1568.223655	18.324659	-0.045766	2.249171
245.183549	1560.249883	18.329664	-0.045802	2.244185
244.948148	1552.337297	18.334669	-0.045753	2.239186
244.880214	1544.407993	18.339674	-0.045735	2.234180
244.874288	1536.427365	18.344679	-0.045728	2.229135
244.849588	1528.480963	18.349683	-0.045718	2.224100
244.722222	1520.570411	18.354688	-0.045689	2.219066
244.734743	1512.596223	18.359693	-0.045686	2.213993
244.738893	1504.655890	18.364698	-0.045681	2.208930
244.693390	1496.702451	18.369703	-0.045667	2.203841
244.518479	1488.798316	18.374707	-0.045629	2.198761
244.617950	1480.832018	18.379712	-0.045643	2.193654
244.345602	1472.869469	18.384717	-0.045586	2.188504
244.489146	1464.915960	18.389722	-0.045608	2.183385
244.507370	1456.966463	18.394727	-0.045606	2.178246
244.451976	1449.039666	18.399731	-0.045590	2.173102
244.223930	1441.106801	18.404736	-0.045542	2.167926
243.926538	1433.188787	18.409741	-0.045481	2.162741
244.157126	1425.239226	18.414746	-0.045519	2.157572
244.189430	1417.278974	18.419751	-0.045519	2.152365
244.054058	1409.350525	18.424755	-0.045489	2.147150
244.140520	1401.388541	18.429760	-0.045499	2.141922
243.993303	1393.475890	18.434765	-0.045467	2.136691
243.844398	1385.559358	18.439770	-0.045433	2.131445
243.886919	1377.591578	18.444775	-0.045436	2.126169
243.930436	1369.653942	18.449779	-0.045439	2.120901
243.501593	1361.784428	18.454784	-0.045353	2.115620
243.339633	1353.772775	18.459789	-0.045318	2.110256
243.524997	1345.802424	18.464794	-0.045347	2.104940
243.366660	1337.878344	18.469799	-0.045312	2.099608
243.361007	1329.961860	18.474803	-0.045305	2.094283
243.303744	1322.014959	18.479808	-0.045289	2.088918
243.237289	1314.082224	18.484813	-0.045272	2.083548
243.333834	1306.166253	18.489818	-0.045284	2.078192
243.163945	1298.249095	18.494823	-0.045247	2.072795
242.976299	1290.326887	18.499827	-0.045207	2.067378
243.131543	1282.372947	18.504832	-0.045230	2.061960
242.743417	1274.487416	18.509837	-0.045153	2.056519
242.922770	1266.520136	18.514842	-0.045181	2.051066
242.701403	1258.610262	18.519847	-0.045134	2.045596
242.662627	1250.692386	18.524851	-0.045121	2.040125
242.827324	1242.758172	18.529856	-0.045147	2.034649
242.761177	1234.786197	18.534861	-0.045129	2.029108
242.606152	1226.877797	18.539866	-0.045095	2.023587
242.440771	1218.967593	18.544871	-0.045058	2.018049
242.578424	1211.009461	18.549875	-0.045079	2.012493
242.493849	1203.096521	18.554880	-0.045057	2.006930
242.386630	1195.178574	18.559885	-0.045032	2.001346
242.458387	1187.263731	18.564890	-0.045040	1.995767
242.313842	1179.332602	18.569895	-0.045008	1.990139
242.305874	1171.403897	18.574899	-0.045001	1.984510
242.312007	1163.488118	18.579904	-0.044996	1.978876
242.168251	1155.582272	18.584909	-0.044964	1.973218
242.175544	1147.657034	18.589914	-0.044960	1.967545
241.786826	1139.790838	18.594919	-0.044883	1.961855
241.908805	1131.846152	18.599923	-0.044900	1.956148
241.776817	1123.916419	18.604928	-0.044870	1.950407
241.685205	1115.959503	18.609933	-0.044847	1.944634
241.787301	1108.044129	18.614938	-0.044861	1.938895
241.845899	1100.097655	18.619943	-0.044866	1.933111
241.678247	1092.200240	18.624947	-0.044830	1.927321
241.611948	1084.301587	18.629952	-0.044812	1.921524
241.594139	1076.392545	18.634957	-0.044803	1.915707
241.396002	1068.503510	18.639962	-0.044761	1.909867
241.222076	1060.591036	18.644967	-0.044723	1.903995
241.361136	1052.668849	18.649971	-0.044744	1.898132
241.253324	1044.763039	18.654976	-0.044718	1.892235
240.954419	1036.865275	18.659981	-0.044657	1.886304
240.977256	1028.960233	18.664986	-0.044656	1.880386
241.013172	1021.049612	18.669991	-0.044657	1.874446
240.892974	1013.127245	18.674995	-0.044630	1.868461
240.960632	1005.208425	18.680000	-0.044637	1.862480
240.824287	997.314728	18.685005	-0.044606	1.856476
240.964302	989.381580	18.690010	-0.044627	1.850455
240.796205	981.487885	18.695015	-0.044590	1.844407
240.613238	973.632034	18.700019	-0.044551	1.838368
240.711897	965.710963	18.705024	-0.044563	1.832291
240.353903	957.842704	18.710029	-0.044491	1.826181
240.392310	949.931491	18.715034	-0.044493	1.820064
240.358822	942.044648	18.720039	-0.044482	1.813936
240.221740	934.140840	18.725043	-0.044451	1.807763
240.438301	926.220557	18.730048	-0.044486	1.801598
240.350297	918.332808	18.735053	-0.044464	1.795400
240.215097	910.407586	18.740058	-0.044433	1.789145
240.082735	902.525106	18.745063	-0.044403	1.782903
240.140712	894.628719	18.750067	-0.044409	1.776651
240.004293	886.745039	18.755072	-0.044378	1.770364
239.909967	878.859659	18.760077	-0.044355	1.764057
239.681874	871.022618	18.765082	-0.044307	1.757750
239.693310	863.118691	18.770087	-0.044304	1.751396
239.429127	855.255998	18.775091	-0.044249	1.745018
239.388857	847.379485	18.780096	-0.044236	1.738634
239.538783	839.451652	18.785101	-0.044259	1.732208
239.506670	831.564821	18.790106	-0.044247	1.725769
239.197529	823.747533	18.795111	-0.044185	1.719327
239.155649	815.859159	18.800115	-0.044171	1.712836
239.247506	807.942588	18.805120	-0.044183	1.706315
238.927412	800.103456	18.810125	-0.044118	1.699780
238.986567	792.226204	18.815130	-0.044124	1.693237
238.902117	784.333504	18.820135	-0.044103	1.686637
238.877021	776.466788	18.825139	-0.044093	1.680041
238.732031	768.640315	18.830144	-0.044060	1.673436
238.611301	760.750236	18.835149	-0.044032	1.666755
238.678764	752.872050	18.840154	-0.044040	1.660082
238.408920	745.051089	18.845159	-0.043984	1.653386
238.484612	737.145763	18.850163	-0.043993	1.646637
238.523552	729.288185	18.855168	-0.043995	1.639896
238.252574	721.450498	18.860173	-0.043939	1.633102
238.277557	713.531029	18.865178	-0.043938	1.626250
238.262100	705.676046	18.870183	-0.043930	1.619419
237.948457	697.865007	18.875187	-0.043866	1.612555
238.012013	689.987702	18.880192	-0.043872	1.605658
237.927207	682.152021	18.885197	-0.043851	1.598746
238.052587	674.291079	18.890202	-0.043869	1.591811
237.805213	666.464756	18.895207	-0.043818	1.584824
237.656651	658.640977	18.900211	-0.043785	1.577823
237.717163	650.784033	18.905216	-0.043791	1.570790
237.500517	642.954836	18.910221	-0.043745	1.563711
237.659848	635.101812	18.915226	-0.043769	1.556632
237.574793	627.254909	18.920231	-0.043748	1.549491
237.460655	619.420070	18.925235	-0.043722	1.542324
237.323593	611.615057	18.930240	-0.043691	1.535147
237.130304	603.785764	18.935245	-0.043649	1.527906
237.231709	595.948127	18.940250	-0.043663	1.520667
236.944567	588.174068	18.945255	-0.043604	1.513393
236.782468	580.340580	18.950259	-0.043569	1.506047
236.823112	572.519930	18.955264	-0.043571	1.498709
236.700011	564.697220	18.960269	-0.043543	1.491308
236.716278	556.876305	18.965274	-0.043540	1.483892
236.594580	549.086915	18.970279	-0.043512	1.476448
236.508245	541.223952	18.975283	-0.043491	1.468902
236.423873	533.421450	18.980288	-0.043470	1.461374
236.137815	525.655636	18.985293	-0.043411	1.453812
236.100430	517.838182	18.990298	-0.043399	1.446199
235.899799	510.077909	18.995303	-0.043356	1.438575
235.741143	502.289771	19.000307	-0.043321	1.430891
235.884663	494.459324	19.005312	-0.043343	1.423172
235.687752	486.695408	19.010317	-0.043301	1.415421
235.453706	478.927352	19.015322	-0.043252	1.407617
235.540302	471.121693	19.020327	-0.043263	1.399786
235.414861	463.353702	19.025331	-0.043234	1.391912
235.281957	455.580872	19.030336	-0.043204	1.383988
235.119840	447.816210	19.035341	-0.043168	1.376021
235.138617	440.034547	19.040346	-0.043167	1.368022
234.669319	432.334906	19.045351	-0.043074	1.359976
234.502191	424.583348	19.050355	-0.043038	1.351881
234.379756	416.828477	19.055360	-0.043009	1.343741
234.270472	409.070254	19.060365	-0.042984	1.335550
234.020094	401.346322	19.065370	-0.042932	1.327320
233.849501	393.615610	19.070375	-0.042895	1.319045
233.632142	385.806783	19.075379	-0.042849	1.310626
233.364511	378.049601	19.080384	-0.042794	1.302198
233.128217	370.339950	19.085389	-0.042745	1.293774
233.210776	362.579734	19.090394	-0.042755	1.285297
232.746594	354.934394	19.095399	-0.042663	1.276790
232.305110	347.263605	19.100403	-0.042576	1.268201
232.013402	339.581372	19.105408	-0.042516	1.259569
231.701673	331.889512	19.110413	-0.042453	1.250862
231.287027	324.234434	19.115418	-0.042370	1.242116
231.022391	316.545951	19.120423	-0.042316	1.233299
230.871984	308.826307	19.125427	-0.042282	1.224405
230.555406	301.172527	19.130432	-0.042218	1.215489
230.091127	293.521110	19.135437	-0.042127	1.206481
230.000867	285.847818	19.140442	-0.042105	1.197454
229.390935	278.238520	19.145447	-0.041986	1.188329
228.736432	270.646240	19.150451	-0.041859	1.179144
228.497807	262.992620	19.155456	-0.041809	1.169899
227.895395	255.394274	19.160461	-0.041692	1.160572
227.420685	247.773941	19.165466	-0.041598	1.151168
227.118150	240.119955	19.170471	-0.041536	1.141682
226.840036	232.491105	19.175475	-0.041479	1.132152
226.407153	224.903994	19.180480	-0.041394	1.122561
225.930533	217.331592	19.185485	-0.041300	1.112896
225.421074	209.770267	19.190490	-0.041200	1.103153
225.046230	202.195527	19.195495	-0.041125	1.093335
224.657621	194.616344	19.200499	-0.041047	1.083420
224.332296	187.062748	19.205504	-0.040981	1.073461
223.711670	179.533560	19.210509	-0.040861	1.063372
223.184324	172.026330	19.215514	-0.040757	1.053238
222.714611	164.497930	19.220519	-0.040665	1.042990
222.458938	156.958298	19.225523	-0.040612	1.032676
221.756530	149.505027	19.230528	-0.040476	1.022269
221.173401	142.037247	19.235533	-0.040362	1.011764
221.097740	134.504254	19.240538	-0.040343	1.001181
220.595416	127.041131	19.245543	-0.040245	0.990478
219.946758	119.605548	19.250547	-0.040119	0.979661
219.481727	112.180085	19.255552	-0.040027	0.968785
218.986184	104.767195	19.260557	-0.039930	0.957795
218.497149	97.366100	19.265562	-0.039834	0.946697
218.010535	89.988192	19.270567	-0.039738	0.935502
217.588349	82.604662	19.275571	-0.039654	0.924180
216.887982	75.297948	19.280576	-0.039519	0.912761
216.295150	67.967720	19.285581	-0.039403	0.901189
215.853618	60.872001	19.290586	-0.039316	0.889881