Fri Mar 12 12:47:52 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.506737	0.120437	0.000000	0.000007	0.718940

0.165009	0.190316	0.005005	0.000071	0.718958
0.189351	0.187008	0.010010	0.000066	0.718959
0.180005	0.186378	0.015014	0.000068	0.718955
0.203421	0.186715	0.020019	0.000064	0.718963
0.198764	0.037552	0.025024	0.000065	0.718667
0.239225	0.016191	0.030029	0.000058	0.718639
0.159195	0.031788	0.035034	0.000073	0.718641
0.237979	0.014988	0.040038	0.000058	0.718636
0.104979	0.041877	0.045043	0.000083	0.718642
0.117897	0.036176	0.050048	0.000081	0.718635
0.204330	0.023982	0.055053	0.000065	0.718641
0.200522	0.026281	0.060058	0.000066	0.718644
0.020399	0.052944	0.065062	0.000099	0.718633
0.440859	-0.017594	0.070067	0.000021	0.718641
0.235758	0.017669	0.075072	0.000060	0.718638
0.256848	0.014307	0.080077	0.000056	0.718639
0.346277	0.000671	0.085082	0.000039	0.718643
0.297697	-0.060133	0.090086	0.000048	0.718506
0.237825	-0.128358	0.095091	0.000060	0.718350
0.343746	-0.149477	0.100096	0.000040	0.718345
0.327625	-0.145501	0.105101	0.000043	0.718347
0.363332	-0.151308	0.110106	0.000037	0.718348
0.267515	-0.137523	0.115110	0.000055	0.718341
0.340681	-0.182327	0.120115	0.000041	0.718278
0.061642	-0.271377	0.125120	0.000093	0.718004
0.134383	-0.280740	0.130125	0.000080	0.718011
0.257174	-0.301505	0.135130	0.000057	0.718013
0.216486	-0.298446	0.140134	0.000065	0.718004
0.303094	-0.341048	0.145139	0.000049	0.717950
0.054038	-0.425937	0.150144	0.000095	0.717695
0.066828	-0.427861	0.155149	0.000093	0.717695
0.105577	-0.433619	0.160154	0.000086	0.717697
0.037975	-0.424540	0.165158	0.000099	0.717691
0.284175	-0.602056	0.170163	0.000053	0.717427
0.207595	-0.615884	0.175168	0.000068	0.717372
0.225829	-0.618226	0.180173	0.000064	0.717374
0.319842	-0.658966	0.185178	0.000047	0.717326
0.157117	-0.758251	0.190182	0.000077	0.717072
0.165145	-0.755539	0.195187	0.000076	0.717080
0.118910	-0.749829	0.200192	0.000085	0.717075
0.010459	-0.865361	0.205197	0.000105	0.716808
0.160572	-0.920925	0.210202	0.000077	0.716750
-0.136196	-0.872006	0.215206	0.000133	0.716742
-0.079170	-0.973828	0.220211	0.000122	0.716560
-0.216530	-1.011284	0.225216	0.000148	0.716438
-0.268192	-1.000623	0.230221	0.000158	0.716440
-0.276318	-1.082171	0.235226	0.000160	0.716276
-0.117627	-1.189515	0.240230	0.000130	0.716119
-0.072625	-1.191741	0.245235	0.000122	0.716130
-0.273155	-1.249022	0.250240	0.000159	0.715946
-0.173326	-1.303590	0.255245	0.000141	0.715872
-0.192549	-1.299615	0.260250	0.000145	0.715873
-0.310665	-1.449294	0.265254	0.000167	0.715535
-0.156785	-1.469740	0.270259	0.000138	0.715548
-0.204952	-1.539879	0.275264	0.000147	0.715392
-0.361892	-1.595856	0.280269	0.000177	0.715225
-0.264527	-1.613832	0.285274	0.000159	0.715224
-0.397837	-1.753608	0.290278	0.000184	0.714899
-0.348394	-1.759781	0.295283	0.000175	0.714904
-0.604998	-1.812099	0.300288	0.000223	0.714709
-0.592700	-1.870156	0.305293	0.000221	0.714598
-0.376931	-1.958323	0.310298	0.000181	0.714499
-0.585563	-2.037756	0.315302	0.000220	0.714267
-0.588549	-2.045986	0.320307	0.000220	0.714250
-1.300887	-2.060656	0.325312	0.000353	0.713968
-2.321985	-1.878185	0.330317	0.000543	0.713969
-2.087132	-2.001593	0.335322	0.000500	0.713807
-3.227330	-1.878346	0.340326	0.000712	0.713647
-2.874624	-1.936986	0.345331	0.000647	0.713656
-2.776906	-2.040949	0.350336	0.000629	0.713483
-4.267562	-1.839012	0.355341	0.000906	0.713356
-3.520233	-1.969967	0.360346	0.000767	0.713361
-3.577213	-2.029852	0.365350	0.000778	0.713221
-4.831746	-1.902081	0.370355	0.001012	0.713030
-4.656459	-1.937353	0.375360	0.000979	0.713022
-5.069290	-1.863483	0.380365	0.001056	0.713022
-4.923069	-2.016000	0.385370	0.001029	0.712770
-5.851456	-1.883553	0.390374	0.001202	0.712705
-5.705319	-1.905514	0.395379	0.001175	0.712712
-5.347783	-1.971650	0.400384	0.001108	0.712707
-5.943780	-2.002481	0.405389	0.001220	0.712434
-6.674036	-1.895090	0.410394	0.001356	0.712389
-6.510586	-1.928799	0.415398	0.001325	0.712379
-6.048736	-2.006037	0.420403	0.001239	0.712389
-6.759642	-1.952868	0.425408	0.001372	0.712243
-7.675564	-1.867419	0.430413	0.001543	0.712087
-6.972411	-1.990400	0.435418	0.001412	0.712092
-7.513283	-1.897784	0.440422	0.001513	0.712084
-7.559708	-1.884773	0.445427	0.001521	0.712093
-7.326659	-2.023185	0.450432	0.001478	0.711900
-8.667954	-1.855398	0.455437	0.001728	0.711758
-8.326085	-1.912127	0.460442	0.001664	0.711766
-8.267365	-1.927523	0.465446	0.001654	0.711756
-8.333611	-1.911921	0.470451	0.001666	0.711763
-8.348511	-1.943284	0.475456	0.001669	0.711695
-9.076647	-1.934508	0.480461	0.001805	0.711454
-8.651101	-2.007051	0.485466	0.001726	0.711460
-9.572269	-1.848774	0.490470	0.001897	0.711448
-9.221868	-1.905891	0.495475	0.001832	0.711458
-8.917836	-1.962533	0.500480	0.001776	0.711453
-9.276874	-1.997540	0.505485	0.001843	0.711255
-10.457131	-1.844681	0.510490	0.002062	0.711141
-10.286814	-1.880155	0.515494	0.002031	0.711130
-9.809819	-1.959992	0.520499	0.001942	0.711140
-10.003428	-1.927642	0.525504	0.001978	0.711136
-9.967818	-1.934417	0.530509	0.001972	0.711135
-9.933214	-2.003861	0.535514	0.001966	0.711008
-11.115648	-1.864587	0.540518	0.002186	0.710865
-10.635330	-1.945762	0.545523	0.002097	0.710874
-10.556425	-1.962677	0.550528	0.002082	0.710868
-10.900029	-1.901407	0.555533	0.002146	0.710868
-10.594921	-1.951046	0.560538	0.002089	0.710877
-10.745044	-2.023547	0.565542	0.002118	0.710679
-11.669871	-1.927562	0.570547	0.002290	0.710541
-11.723974	-1.921632	0.575552	0.002300	0.710533
-11.955074	-1.881465	0.580557	0.002343	0.710531
-11.727076	-1.919438	0.585562	0.002301	0.710536
-11.845965	-1.902705	0.590566	0.002323	0.710527
-11.897167	-1.909445	0.595571	0.002333	0.710495
-12.537842	-1.933803	0.600576	0.002452	0.710218
-12.578380	-1.927828	0.605581	0.002460	0.710215
-12.914987	-1.864482	0.610586	0.002523	0.710222
-12.952829	-1.862386	0.615590	0.002530	0.710212
-12.509787	-1.938411	0.620595	0.002447	0.710218
-12.895659	-1.870464	0.625600	0.002519	0.710216
-12.681142	-1.940485	0.630605	0.002480	0.710152
-13.264331	-1.966115	0.635610	0.002588	0.709893
-13.656681	-1.899901	0.640614	0.002661	0.709885
-13.902517	-1.852302	0.645619	0.002707	0.709893
-13.406520	-1.940773	0.650624	0.002615	0.709892
-13.269848	-1.966964	0.655629	0.002590	0.709888
-13.603487	-1.904655	0.660634	0.002652	0.709894
-13.589919	-1.965238	0.665638	0.002650	0.709777
-14.312283	-1.927008	0.670643	0.002784	0.709596
-14.304796	-1.927834	0.675648	0.002783	0.709597
-14.642262	-1.868667	0.680653	0.002846	0.709595
-14.212435	-1.943357	0.685658	0.002766	0.709598
-14.232686	-1.942791	0.690662	0.002770	0.709592
-14.674017	-1.861640	0.695667	0.002852	0.709597
-14.415059	-2.009275	0.700672	0.002804	0.709393
-15.404599	-1.898334	0.705677	0.002988	0.709262
-15.165693	-1.936348	0.710682	0.002944	0.709271
-15.502109	-1.883568	0.715686	0.003007	0.709257
-15.303259	-1.916120	0.720691	0.002970	0.709262
-15.345682	-1.907857	0.725696	0.002978	0.709263
-15.653650	-1.852814	0.730701	0.003035	0.709263
-15.382364	-1.987936	0.735706	0.002985	0.709090
-16.470028	-1.863411	0.740710	0.003188	0.708951
-16.316952	-1.886131	0.745715	0.003159	0.708959
-16.173125	-1.914999	0.750720	0.003133	0.708953
-16.099201	-1.928213	0.755725	0.003119	0.708952
-16.217099	-1.903613	0.760730	0.003141	0.708959
-16.408395	-1.872521	0.765734	0.003177	0.708953
-16.296358	-1.966475	0.770739	0.003156	0.708805
-17.136549	-1.898572	0.775744	0.003313	0.708641
-17.281100	-1.875107	0.780749	0.003340	0.708636
-16.953735	-1.929829	0.785754	0.003279	0.708643
-17.144440	-1.900164	0.790758	0.003315	0.708634
-17.098625	-1.905523	0.795763	0.003306	0.708639
-17.036755	-1.916861	0.800768	0.003295	0.708638
-17.381824	-1.920741	0.805773	0.003359	0.708507
-17.965729	-1.894036	0.810778	0.003468	0.708352
-17.927011	-1.903858	0.815782	0.003461	0.708346
-17.783008	-1.927965	0.820787	0.003434	0.708349
-17.815502	-1.921394	0.825792	0.003440	0.708350
-18.013507	-1.887777	0.830797	0.003477	0.708346
-17.761674	-1.928766	0.835802	0.003431	0.708354
-18.071096	-1.983442	0.840806	0.003488	0.708134
-19.031228	-1.872038	0.845811	0.003667	0.708014
-18.766289	-1.919726	0.850816	0.003618	0.708013
-18.859957	-1.904393	0.855821	0.003636	0.708010
-18.601561	-1.946515	0.860826	0.003588	0.708017
-18.904410	-1.896584	0.865830	0.003644	0.708009
-18.688407	-1.931891	0.870835	0.003604	0.708015
-18.754951	-2.040854	0.875840	0.003617	0.707773
-20.225425	-1.818449	0.880845	0.003890	0.707693
-19.731335	-1.900990	0.885850	0.003799	0.707704
-19.585112	-1.932227	0.890854	0.003771	0.707693
-19.939208	-1.867244	0.895859	0.003837	0.707696
-19.913810	-1.870214	0.900864	0.003833	0.707699
-19.772761	-1.898856	0.905869	0.003807	0.707692
-19.793959	-1.987212	0.910874	0.003811	0.707507
-21.085421	-1.826955	0.915878	0.004051	0.707366
-20.687363	-1.894950	0.920883	0.003977	0.707372
-20.345910	-1.955344	0.925888	0.003914	0.707373
-20.853847	-1.867607	0.930893	0.004009	0.707367
-20.474720	-1.929349	0.935898	0.003938	0.707379
-20.415776	-1.945883	0.940902	0.003927	0.707366
-20.848895	-1.941289	0.945907	0.004008	0.707220
-21.561856	-1.882871	0.950912	0.004141	0.707082
-21.481680	-1.899766	0.955917	0.004126	0.707077
-21.084236	-1.965360	0.960922	0.004052	0.707087
-21.719481	-1.856171	0.965926	0.004171	0.707079
-21.683728	-1.861843	0.970931	0.004164	0.707080
-21.183743	-1.951858	0.975936	0.004071	0.707078
-21.699109	-1.942444	0.980941	0.004167	0.706912
-22.532376	-1.871950	0.985946	0.004323	0.706755
-22.267748	-1.923433	0.990950	0.004273	0.706746
-22.418938	-1.892130	0.995955	0.004302	0.706755
-22.548561	-1.871083	1.000960	0.004326	0.706750
-22.186746	-1.936898	1.005965	0.004259	0.706747
-22.080661	-1.951804	1.010970	0.004239	0.706755
-22.606025	-1.940100	1.015974	0.004337	0.706590
-23.298976	-1.890539	1.020979	0.004466	0.706442
-22.931747	-1.954794	1.025984	0.004398	0.706444
-23.635672	-1.832810	1.030989	0.004529	0.706436
-23.474889	-1.856808	1.035994	0.004499	0.706446
-23.024195	-1.938855	1.040998	0.004416	0.706442
-23.308351	-1.886259	1.046003	0.004469	0.706446
-23.136054	-1.985909	1.051008	0.004437	0.706307
-24.175321	-1.892361	1.056013	0.004630	0.706122
-23.769269	-1.960434	1.061018	0.004555	0.706131
-24.284171	-1.873809	1.066022	0.004651	0.706120
-24.333373	-1.861660	1.071027	0.004660	0.706127
-23.901279	-1.940120	1.076032	0.004580	0.706123
-24.182602	-1.890475	1.081037	0.004632	0.706122
-24.216457	-1.954313	1.086042	0.004639	0.705981
-25.015567	-1.872057	1.091046	0.004787	0.705860
-25.038156	-1.866865	1.096051	0.004792	0.705862
-25.042500	-1.865817	1.101056	0.004793	0.705863
-25.204943	-1.838993	1.106061	0.004823	0.705858
-24.834127	-1.900011	1.111066	0.004754	0.705868
-25.185533	-1.840898	1.116070	0.004820	0.705861
-25.465404	-1.838309	1.121075	0.004872	0.705765
-25.895330	-1.880574	1.126080	0.004952	0.705526
-25.725989	-1.914174	1.131085	0.004921	0.705519
-25.946552	-1.868764	1.136090	0.004962	0.705531
-25.872009	-1.886783	1.141094	0.004948	0.705521
-25.688809	-1.917540	1.146099	0.004914	0.705525
-26.021059	-1.857378	1.151104	0.004976	0.705526
-26.043424	-1.898537	1.156109	0.004980	0.705435
-26.755119	-1.881866	1.161114	0.005113	0.705213
-26.884627	-1.861684	1.166118	0.005137	0.705207
-27.069337	-1.827165	1.171123	0.005172	0.705210
-26.636656	-1.903019	1.176128	0.005091	0.705212
-26.870915	-1.864047	1.181133	0.005135	0.705207
-27.070226	-1.825219	1.186138	0.005172	0.705213
-26.870109	-1.863103	1.191142	0.005135	0.705208
-27.417971	-1.919043	1.196147	0.005237	0.704899
-27.941505	-1.830824	1.201152	0.005335	0.704888
-28.213718	-1.784502	1.206157	0.005386	0.704883
-27.445760	-1.916953	1.211162	0.005243	0.704892
-27.911585	-1.836154	1.216166	0.005330	0.704887
-28.229235	-1.778012	1.221171	0.005389	0.704890
-27.698307	-1.872894	1.226176	0.005290	0.704890
-27.932619	-1.894590	1.231181	0.005334	0.704761
-28.941579	-1.796725	1.236186	0.005522	0.704596
-28.472445	-1.885280	1.241190	0.005435	0.704586
-28.566032	-1.866889	1.246195	0.005452	0.704589
-28.681871	-1.843989	1.251200	0.005474	0.704593
-28.722030	-1.841709	1.256205	0.005482	0.704583
-28.597165	-1.858894	1.261210	0.005459	0.704593
-28.523807	-1.938743	1.266214	0.005445	0.704459
-29.743234	-1.821550	1.271219	0.005672	0.704256
-29.225691	-1.911185	1.276224	0.005576	0.704261
-29.407110	-1.882015	1.281229	0.005610	0.704255
-29.414912	-1.876557	1.286234	0.005611	0.704263
-29.323023	-1.895919	1.291238	0.005594	0.704256
-29.308874	-1.897859	1.296243	0.005592	0.704257
-29.638111	-1.945340	1.301248	0.005653	0.704043
-30.605310	-1.821468	1.306253	0.005834	0.703945
-30.062882	-1.912293	1.311258	0.005733	0.703956
-30.075017	-1.912140	1.316262	0.005735	0.703952
-30.817427	-1.781131	1.321267	0.005873	0.703949
-30.350439	-1.860749	1.326272	0.005787	0.703956
-30.128227	-1.904738	1.331277	0.005745	0.703947
-30.531101	-1.954979	1.336282	0.005821	0.703701
-31.176144	-1.874630	1.341286	0.005941	0.703631
-31.177889	-1.873389	1.346291	0.005941	0.703632
-30.899302	-1.921703	1.351296	0.005889	0.703635
-31.345335	-1.845350	1.356301	0.005973	0.703628
-30.866918	-1.926855	1.361306	0.005884	0.703636
-30.829805	-1.965767	1.366310	0.005877	0.703570
-32.080641	-1.855819	1.371315	0.006110	0.703342
-31.663666	-1.927146	1.376320	0.006032	0.703348
-31.991255	-1.872642	1.381325	0.006093	0.703339
-32.179087	-1.836792	1.386330	0.006129	0.703344
-32.168449	-1.840388	1.391334	0.006127	0.703340
-32.008870	-1.868336	1.396339	0.006097	0.703341
-31.715875	-1.983782	1.401344	0.006043	0.703213
-33.093475	-1.842859	1.406349	0.006299	0.703002
-32.583987	-1.929989	1.411354	0.006205	0.703009
-32.807751	-1.892718	1.416358	0.006246	0.703003
-33.154619	-1.830058	1.421363	0.006311	0.703005
-32.864773	-1.879263	1.426368	0.006257	0.703009
-32.787950	-1.898252	1.431373	0.006243	0.702998
-32.920831	-1.955081	1.436378	0.006268	0.702836
-34.081067	-1.819749	1.441382	0.006484	0.702691
-33.391968	-1.940916	1.446387	0.006356	0.702694
-33.150380	-1.981788	1.451392	0.006311	0.702698
-33.874199	-1.858135	1.456397	0.006446	0.702687
-33.575553	-1.905936	1.461402	0.006390	0.702698
-33.467919	-1.929220	1.466406	0.006371	0.702689
-34.153205	-1.955858	1.471411	0.006498	0.702388
-34.441600	-1.910997	1.476416	0.006552	0.702375
-34.709944	-1.869093	1.481421	0.006602	0.702363
-34.450373	-1.909120	1.486426	0.006554	0.702375
-34.666238	-1.874875	1.491430	0.006594	0.702366
-34.535550	-1.896052	1.496435	0.006570	0.702370
-34.161230	-1.985031	1.501440	0.006501	0.702325
-35.254739	-1.918846	1.506445	0.006704	0.702064
-35.180752	-1.926518	1.511450	0.006691	0.702075
-35.213132	-1.921630	1.516454	0.006697	0.702073
-35.227568	-1.920173	1.521459	0.006700	0.702071
-35.324063	-1.899068	1.526464	0.006718	0.702078
-35.466569	-1.878826	1.531469	0.006744	0.702068
-35.330252	-1.993458	1.536474	0.006719	0.701885
-36.576613	-1.842075	1.541478	0.006951	0.701741
-36.523990	-1.850029	1.546483	0.006942	0.701744
-36.172063	-1.910852	1.551488	0.006876	0.701747
-36.531837	-1.850593	1.556493	0.006943	0.701739
-36.326290	-1.883232	1.561498	0.006905	0.701747
-35.981790	-1.946819	1.566502	0.006841	0.701743
-36.408775	-1.934778	1.571507	0.006921	0.701613
-37.452366	-1.834247	1.576512	0.007115	0.701439
-37.099625	-1.901155	1.581517	0.007050	0.701431
-37.141459	-1.888874	1.586522	0.007058	0.701440
-37.424867	-1.842190	1.591526	0.007110	0.701432
-37.060238	-1.907285	1.596531	0.007043	0.701432
-36.970055	-1.919548	1.601536	0.007026	0.701439
-37.163884	-1.943116	1.606541	0.007062	0.701322
-37.901204	-1.909567	1.611546	0.007200	0.701123
-37.749009	-1.938824	1.616550	0.007171	0.701118
-38.227631	-1.853743	1.621555	0.007261	0.701118
-37.994409	-1.892786	1.626560	0.007217	0.701123
-38.009714	-1.895604	1.631565	0.007220	0.701111
-37.914664	-1.906000	1.636570	0.007203	0.701124
-38.172326	-1.924630	1.641574	0.007251	0.700993
-38.862296	-1.862265	1.646579	0.007379	0.700870
-38.386796	-1.943359	1.651584	0.007291	0.700877
-38.766373	-1.881061	1.656589	0.007362	0.700866
-38.897454	-1.854217	1.661594	0.007386	0.700873
-38.428940	-1.937686	1.666598	0.007299	0.700873
-38.542385	-1.938177	1.671603	0.007320	0.700831
-39.622901	-1.890326	1.676608	0.007522	0.700537
-39.737937	-1.874429	1.681613	0.007543	0.700527
-39.624433	-1.891434	1.686618	0.007522	0.700533
-39.474089	-1.919398	1.691622	0.007494	0.700531
-39.710077	-1.876811	1.696627	0.007538	0.700532
-39.378165	-1.931379	1.701632	0.007477	0.700541
-39.657989	-1.941071	1.706637	0.007529	0.700420
-40.586888	-1.874949	1.711642	0.007702	0.700218
-40.344137	-1.917583	1.716646	0.007657	0.700219
-40.551369	-1.881471	1.721651	0.007696	0.700217
-40.417230	-1.901735	1.726656	0.007671	0.700224
-40.555887	-1.880815	1.731661	0.007697	0.700216
-40.533487	-1.881305	1.736666	0.007693	0.700223
-40.592884	-1.941897	1.741670	0.007704	0.700078
-41.786227	-1.822098	1.746675	0.007926	0.699889
-41.114260	-1.938125	1.751680	0.007801	0.699897
-41.440806	-1.885234	1.756685	0.007862	0.699886
-41.613556	-1.850693	1.761690	0.007894	0.699893
-41.069151	-1.947586	1.766694	0.007793	0.699893
-41.255790	-1.915491	1.771699	0.007828	0.699891
-41.387393	-1.975400	1.776704	0.007853	0.699721
-42.456859	-1.847382	1.781709	0.008052	0.699594
-41.990460	-1.927251	1.786714	0.007965	0.699600
-41.832956	-1.957338	1.791718	0.007936	0.699596
-42.419016	-1.854086	1.796723	0.008045	0.699593
-41.957586	-1.932800	1.801728	0.007960	0.699600
-42.146860	-1.902002	1.806733	0.007995	0.699594
-42.618740	-1.969176	1.811738	0.008083	0.699286
-42.995775	-1.911078	1.816742	0.008153	0.699267
-43.248269	-1.868273	1.821747	0.008200	0.699263
-43.050483	-1.900855	1.826752	0.008164	0.699268
-43.214888	-1.875836	1.831757	0.008194	0.699259
-42.764134	-1.952649	1.836762	0.008111	0.699266
-42.808826	-1.977954	1.841766	0.008119	0.699198
-44.014746	-1.883817	1.846771	0.008344	0.698952
-43.654845	-1.944546	1.851776	0.008277	0.698959
-43.627395	-1.954432	1.856781	0.008272	0.698949
-43.983344	-1.887836	1.861786	0.008338	0.698955
-43.973200	-1.889681	1.866790	0.008336	0.698954
-43.952582	-1.893932	1.871795	0.008333	0.698953
-43.682252	-2.012887	1.876800	0.008283	0.698809
-45.013831	-1.862672	1.881805	0.008531	0.698631
-44.453825	-1.959669	1.886810	0.008426	0.698637
-44.515138	-1.949998	1.891814	0.008438	0.698634
-45.138129	-1.839728	1.896819	0.008554	0.698632
-44.660876	-1.919969	1.901824	0.008465	0.698642
-44.646166	-1.927850	1.906829	0.008463	0.698631
-45.109424	-1.937735	1.911834	0.008549	0.698443
-45.712254	-1.876576	1.916838	0.008661	0.698348
-45.449563	-1.925613	1.921843	0.008613	0.698343
-45.225200	-1.959986	1.926848	0.008571	0.698355
-45.783017	-1.866173	1.931853	0.008675	0.698343
-45.422117	-1.926049	1.936858	0.008608	0.698352
-45.391360	-1.932223	1.941862	0.008602	0.698350
-46.342627	-1.929140	1.946867	0.008780	0.698011
-46.444791	-1.907962	1.951872	0.008799	0.698017
-46.572749	-1.889893	1.956877	0.008823	0.698007
-46.493939	-1.901185	1.961882	0.008808	0.698012
-46.580131	-1.885003	1.966886	0.008824	0.698014
-46.702330	-1.865737	1.971891	0.008847	0.698008
-46.301308	-1.932773	1.976896	0.008773	0.698017
-47.020691	-1.941940	1.981901	0.008907	0.697737
-47.592247	-1.858089	1.986906	0.009013	0.697700
-47.391534	-1.894346	1.991910	0.008976	0.697699
-47.559753	-1.864952	1.996915	0.009007	0.697697
-47.417680	-1.888303	2.001920	0.008981	0.697701

-47.400738	-1.890897	2.011917	0.008978	0.697702
-47.807677	-1.934871	2.021914	0.009054	0.697464
-48.128104	-1.920228	2.031910	0.009114	0.697377
-48.003805	-1.942432	2.041907	0.009091	0.697376
-48.166383	-1.912777	2.051904	0.009122	0.697377
-48.127702	-1.918712	2.061901	0.009115	0.697378
-48.132847	-1.917712	2.071898	0.009116	0.697378
-48.000136	-1.864517	2.081894	0.009092	0.697534
-47.066631	-1.950068	2.091891	0.008918	0.697699
-47.285285	-1.911101	2.101888	0.008959	0.697698
-47.163525	-1.931048	2.111885	0.008937	0.697701
-47.265156	-1.913492	2.121882	0.008956	0.697700
-47.543077	-1.864684	2.131878	0.009008	0.697697
-47.341517	-1.900323	2.141875	0.008970	0.697698
-47.378874	-1.890200	2.151872	0.008978	0.697704
-47.019303	-1.859498	2.161869	0.008911	0.697897
-46.525989	-1.890493	2.171866	0.008819	0.698012
-46.793863	-1.841635	2.181862	0.008869	0.698014
-46.266804	-1.935521	2.191859	0.008772	0.698014
-46.606942	-1.818619	2.201856	0.008835	0.698128
-45.354690	-1.933163	2.211853	0.008602	0.698349
-45.565085	-1.893366	2.221850	0.008642	0.698353
-45.475120	-1.908946	2.231846	0.008625	0.698353
-45.272881	-1.945665	2.241843	0.008588	0.698351
-45.015980	-1.851853	2.251840	0.008540	0.698635
-44.635257	-1.917214	2.261837	0.008469	0.698639
-44.545234	-1.934688	2.271834	0.008453	0.698636
-44.697694	-1.883926	2.281830	0.008482	0.698684
-44.027911	-1.870104	2.291827	0.008357	0.698954
-43.913537	-1.889652	2.301824	0.008336	0.698955
-43.659938	-1.935184	2.311821	0.008289	0.698954
-43.439173	-1.878159	2.321818	0.008248	0.699150
-43.185871	-1.867004	2.331814	0.008201	0.699263
-42.916877	-1.913588	2.341811	0.008151	0.699266
-43.024441	-1.881818	2.351808	0.008172	0.699291
-42.107230	-1.893057	2.361805	0.008001	0.699600
-42.018508	-1.909491	2.371802	0.007985	0.699598
-42.007679	-1.913728	2.381798	0.007983	0.699593
-41.998047	-1.858963	2.391795	0.007982	0.699707
-41.241423	-1.901435	2.401792	0.007841	0.699894
-41.204368	-1.907693	2.411789	0.007834	0.699894
-41.300459	-1.889743	2.421786	0.007852	0.699896
-40.621929	-1.864553	2.431782	0.007726	0.700192
-40.433002	-1.886297	2.441779	0.007691	0.700215
-40.551332	-1.864497	2.451776	0.007714	0.700216
-39.860979	-1.894922	2.461773	0.007585	0.700404
-39.580851	-1.881271	2.471770	0.007533	0.700532
-39.525981	-1.890281	2.481766	0.007523	0.700533
-39.513916	-1.893547	2.491763	0.007521	0.700531
-38.854615	-1.843378	2.501760	0.007399	0.700870
-38.510322	-1.903228	2.511757	0.007335	0.700873
-38.856369	-1.840628	2.521754	0.007400	0.700874
-38.385427	-1.857834	2.531750	0.007312	0.701009
-38.106212	-1.854881	2.541747	0.007261	0.701115
-37.890086	-1.890716	2.551744	0.007221	0.701120
-37.773645	-1.860078	2.561741	0.007199	0.701224
-37.024242	-1.890270	2.571738	0.007060	0.701433
-36.991913	-1.897306	2.581734	0.007054	0.701430
-37.080366	-1.881606	2.591731	0.007071	0.701429
-36.407734	-1.861196	2.601728	0.006946	0.701713
-36.257571	-1.872869	2.611725	0.006918	0.701743
-36.227956	-1.878996	2.621722	0.006913	0.701741
-35.822714	-1.852332	2.631718	0.006838	0.701940
-35.422109	-1.859550	2.641715	0.006763	0.702070
-35.379406	-1.866234	2.651712	0.006756	0.702071
-35.247972	-1.860377	2.661709	0.006731	0.702130
-34.419513	-1.889480	2.671706	0.006577	0.702369
-34.394730	-1.893277	2.681702	0.006573	0.702370
-34.515055	-1.872670	2.691699	0.006596	0.702368
-33.987472	-1.858019	2.701696	0.006498	0.702587
-33.640272	-1.868683	2.711693	0.006433	0.702690
-33.709495	-1.854403	2.721690	0.006446	0.702694
-33.340212	-1.873251	2.731686	0.006378	0.702788
-32.606100	-1.895624	2.741683	0.006241	0.703007
-32.724963	-1.874931	2.751680	0.006264	0.703006
-32.734708	-1.871179	2.761677	0.006266	0.703009
-32.125865	-1.849000	2.771674	0.006153	0.703273
-31.674443	-1.895109	2.781670	0.006069	0.703342
-31.880249	-1.859225	2.791667	0.006107	0.703340
-31.569679	-1.885753	2.801664	0.006050	0.703397
-30.940644	-1.878522	2.811661	0.005933	0.703638
-30.852965	-1.894113	2.821658	0.005917	0.703637
-30.848872	-1.896273	2.831654	0.005916	0.703634
-30.395473	-1.882245	2.841651	0.005832	0.703825
-29.954335	-1.898902	2.851648	0.005750	0.703949
-30.016847	-1.885391	2.861645	0.005762	0.703954
-29.953063	-1.888429	2.871642	0.005751	0.703970
-29.386931	-1.845960	2.881638	0.005645	0.704259
-29.280569	-1.865967	2.891635	0.005626	0.704256
-29.022976	-1.909990	2.901632	0.005578	0.704260
-28.883694	-1.820907	2.911629	0.005552	0.704489
-28.084265	-1.912507	2.921626	0.005404	0.704591
-28.299302	-1.874711	2.931622	0.005444	0.704589
-28.329869	-1.844475	2.941619	0.005450	0.704639
-27.429834	-1.881913	2.951616	0.005283	0.704886
-27.566640	-1.856629	2.961613	0.005308	0.704887
-27.536537	-1.861761	2.971610	0.005303	0.704887
-26.844710	-1.848601	2.981606	0.005174	0.705162
-26.566427	-1.873443	2.991603	0.005123	0.705211
-26.524269	-1.880219	3.001600	0.005115	0.705212
-26.504758	-1.826043	3.011597	0.005112	0.705328
-25.290278	-1.944842	3.021594	0.004886	0.705524
-25.609835	-1.888612	3.031590	0.004946	0.705522
-25.672349	-1.876339	3.041587	0.004958	0.705524
-24.949007	-1.894422	3.051584	0.004823	0.705746
-24.904804	-1.843436	3.061581	0.004815	0.705864
-24.531552	-1.909389	3.071578	0.004746	0.705865
-24.943345	-1.823622	3.081574	0.004823	0.705889
-23.971063	-1.881160	3.091571	0.004642	0.706122
-23.919035	-1.886585	3.101568	0.004633	0.706129
-23.980115	-1.874840	3.111565	0.004644	0.706130
-23.460797	-1.857577	3.121562	0.004548	0.706351
-23.180415	-1.861045	3.131558	0.004496	0.706444
-23.079593	-1.878743	3.141555	0.004477	0.706444
-23.031071	-1.831772	3.151552	0.004469	0.706555
-22.201083	-1.879738	3.161549	0.004314	0.706755
-21.969505	-1.922027	3.171546	0.004271	0.706753
-22.128369	-1.894447	3.181542	0.004301	0.706751
-21.596368	-1.867858	3.191539	0.004202	0.706994
-21.431127	-1.852780	3.201536	0.004172	0.707083
-21.034191	-1.922753	3.211533	0.004098	0.707084
-21.306210	-1.844639	3.221530	0.004149	0.707143
-20.569063	-1.860074	3.231526	0.004012	0.707375
-20.225734	-1.920608	3.241523	0.003948	0.707376
-20.245878	-1.916470	3.251520	0.003952	0.707377
-19.938317	-1.859110	3.261517	0.003895	0.707602
-19.442657	-1.898092	3.271514	0.003803	0.707700
-19.736247	-1.846463	3.281510	0.003858	0.707698
-19.278103	-1.900223	3.291507	0.003773	0.707754
-18.572224	-1.895940	3.301504	0.003642	0.708014
-18.358083	-1.932626	3.311501	0.003602	0.708017
-18.525290	-1.904927	3.321498	0.003634	0.708012
-18.390287	-1.839475	3.331494	0.003609	0.708191
-17.581485	-1.904389	3.341491	0.003459	0.708349
-17.885687	-1.848687	3.351488	0.003515	0.708352
-17.739048	-1.863746	3.361485	0.003488	0.708373
-17.030083	-1.856885	3.371482	0.003357	0.708640
-17.108550	-1.843367	3.381478	0.003371	0.708638
-17.056042	-1.853037	3.391475	0.003362	0.708637
-16.583685	-1.807153	3.401472	0.003274	0.708897
-16.050058	-1.872241	3.411469	0.003175	0.708957
-16.048514	-1.873062	3.421466	0.003175	0.708955
-16.031720	-1.812654	3.431462	0.003172	0.709082
-14.892516	-1.925914	3.441459	0.002960	0.709261
-15.333687	-1.845100	3.451456	0.003043	0.709265
-14.874796	-1.926688	3.461453	0.002958	0.709265
-14.464098	-1.862697	3.471450	0.002881	0.709539
-14.375869	-1.850797	3.481446	0.002865	0.709594
-14.110239	-1.898214	3.491443	0.002816	0.709593
-14.300477	-1.822148	3.501440	0.002851	0.709677
-13.215576	-1.909147	3.511437	0.002650	0.709889
-13.539901	-1.850604	3.521434	0.002710	0.709890
-13.651025	-1.831347	3.531430	0.002731	0.709889
-12.918311	-1.812062	3.541427	0.002595	0.710188
-12.741525	-1.829801	3.551424	0.002562	0.710215
-12.508242	-1.871648	3.561421	0.002519	0.710214
-12.380006	-1.798984	3.571418	0.002496	0.710404
-11.573164	-1.880054	3.581414	0.002346	0.710529
-11.622059	-1.870871	3.591411	0.002355	0.710529
-11.644005	-1.866412	3.601408	0.002359	0.710530
-11.017029	-1.810286	3.611405	0.002243	0.710865
-10.962150	-1.818539	3.621402	0.002233	0.710867
-10.495927	-1.901816	3.631398	0.002146	0.710866
-10.528983	-1.839002	3.641395	0.002153	0.710980
-9.916404	-1.869575	3.651392	0.002039	0.711136
-9.921036	-1.867809	3.661389	0.002040	0.711137
-10.357847	-1.776655	3.671386	0.002122	0.711163
-9.069218	-1.860684	3.681382	0.001882	0.711453
-9.136717	-1.847402	3.691379	0.001895	0.711455
-9.053391	-1.862055	3.701376	0.001879	0.711455
-8.767758	-1.817967	3.711373	0.001826	0.711644
-8.406125	-1.823106	3.721370	0.001759	0.711762
-8.174822	-1.866204	3.731366	0.001717	0.711758
-8.364517	-1.795711	3.741363	0.001752	0.711831
-7.192170	-1.874435	3.751360	0.001534	0.712090
-6.836611	-1.937909	3.761357	0.001468	0.712089
-6.882482	-1.928912	3.771354	0.001477	0.712090
-6.926476	-1.897229	3.781350	0.001485	0.712137
-6.219176	-1.899812	3.791347	0.001354	0.712383
-6.080733	-1.922715	3.801344	0.001328	0.712386
-5.939964	-1.948112	3.811341	0.001302	0.712385
-6.030416	-1.885853	3.821338	0.001319	0.712476
-5.147422	-1.927174	3.831334	0.001155	0.712706
-5.284788	-1.902856	3.841331	0.001181	0.712706
-5.110215	-1.933687	3.851328	0.001149	0.712706
-4.787838	-1.904330	3.861325	0.001089	0.712878
-4.300382	-1.919089	3.871322	0.000999	0.713021
-4.241097	-1.929850	3.881318	0.000988	0.713020
-4.206552	-1.935809	3.891315	0.000982	0.713020
-3.552340	-1.923618	3.901312	0.000860	0.713276
-3.493108	-1.891074	3.911309	0.000849	0.713361
-3.348236	-1.918930	3.921306	0.000823	0.713357
-3.145673	-1.954196	3.931302	0.000785	0.713358
-2.816765	-1.865074	3.941299	0.000724	0.713651
-2.295194	-1.958434	3.951296	0.000627	0.713650
-2.494517	-1.921743	3.961293	0.000665	0.713652
-2.356763	-1.873718	3.971290	0.000639	0.713795
-1.889779	-1.872813	3.981286	0.000552	0.713962
-2.052069	-1.844805	3.991283	0.000583	0.713960
-1.862429	-1.829669	4.001280	0.000548	0.714057
-1.572907	-1.770283	4.011277	0.000494	0.714277
-1.615818	-1.763269	4.021274	0.000502	0.714275
-1.583458	-1.674995	4.031270	0.000496	0.714461
-1.619680	-1.596166	4.041267	0.000503	0.714604
-1.393973	-1.593472	4.051264	0.000462	0.714689
-1.228334	-1.512781	4.061261	0.000431	0.714907
-1.109324	-1.511538	4.071258	0.000409	0.714952
-0.978956	-1.393244	4.081254	0.000385	0.715232
-1.116387	-1.340081	4.091251	0.000411	0.715288
-0.943092	-1.239772	4.101248	0.000379	0.715548
-0.843906	-1.193824	4.111245	0.000360	0.715674
-0.822631	-1.092545	4.121242	0.000357	0.715881
-0.734576	-1.019264	4.131238	0.000340	0.716057
-0.598678	-0.985057	4.141235	0.000315	0.716173
-0.592483	-0.848462	4.151232	0.000314	0.716445
-0.611175	-0.742635	4.161229	0.000318	0.716647
-0.594313	-0.647850	4.171226	0.000315	0.716840
-0.468190	-0.550936	4.181222	0.000292	0.717076
-0.548918	-0.395919	4.191219	0.000307	0.717354
-0.498470	-0.282791	4.201216	0.000298	0.717595
-0.517886	-0.149389	4.211213	0.000302	0.717851
-0.416413	-0.027504	4.221210	0.000283	0.718127
-0.067288	0.049297	4.231206	0.000218	0.718402
-0.129020	0.191017	4.241203	0.000230	0.718659
0.000000	0.374022	4.251200	0.000206	0.719065

0.071513	0.980564	4.256205	0.000192	0.720286
0.383052	2.169825	4.261210	0.000133	0.722733
0.490457	4.000761	4.266214	0.000112	0.726356
0.613066	6.375951	4.271219	0.000088	0.731023
1.095869	9.200895	4.276224	-0.000003	0.736650
1.429872	12.523731	4.281229	-0.000068	0.743135
1.873907	16.289434	4.286234	-0.000153	0.750439
2.214102	20.483621	4.291238	-0.000219	0.758439
2.704224	25.034150	4.296243	-0.000313	0.767065
3.235315	29.967154	4.301248	-0.000415	0.776307
3.658412	35.248327	4.306253	-0.000497	0.786034
4.125949	40.858560	4.311258	-0.000587	0.796242
4.701893	46.734939	4.316262	-0.000698	0.806823
5.090304	52.943176	4.321267	-0.000775	0.817785
5.544497	59.407593	4.326272	-0.000863	0.829060
6.689359	65.973100	4.331277	-0.001081	0.840559
8.936278	72.601030	4.336282	-0.001503	0.852331
9.502936	79.739430	4.341286	-0.001613	0.864293
9.959232	87.082912	4.346291	-0.001703	0.876391
10.926295	94.509555	4.351296	-0.001888	0.888601
11.948154	102.089946	4.356301	-0.002083	0.900902
13.009820	109.825161	4.361306	-0.002285	0.913288
13.873531	117.707260	4.366310	-0.002451	0.925679
14.726493	125.712189	4.371315	-0.002615	0.938090
15.795343	133.803226	4.376320	-0.002819	0.950522
16.791022	141.978944	4.381325	-0.003010	0.962899
17.742047	150.264069	4.386330	-0.003192	0.975266
18.625679	158.631464	4.391334	-0.003362	0.987579
19.296645	167.093127	4.396339	-0.003492	0.999821
20.391114	175.524442	4.401344	-0.003702	1.011975
21.153197	184.048090	4.406349	-0.003849	1.024033
21.816446	192.639034	4.411354	-0.003978	1.036018
22.697197	201.204730	4.416358	-0.004147	1.047882
23.258971	209.860038	4.421363	-0.004257	1.059660
23.937431	218.522313	4.426368	-0.004389	1.071343
24.616164	227.163911	4.431373	-0.004521	1.082873
25.391858	235.819725	4.436378	-0.004671	1.094321
26.137000	244.469856	4.441382	-0.004815	1.105636
26.872544	253.129015	4.446387	-0.004958	1.116845
27.519523	261.781921	4.451392	-0.005084	1.127916
28.134509	270.444782	4.456397	-0.005204	1.138884
29.016141	279.078865	4.461402	-0.005374	1.149768
29.862981	287.707513	4.466406	-0.005537	1.160536
30.317249	296.365059	4.471411	-0.005627	1.171158
30.880170	305.006954	4.476416	-0.005737	1.181688
31.435092	313.626347	4.481421	-0.005846	1.192096
32.245570	322.189856	4.486426	-0.006002	1.202399
32.873277	330.786897	4.491430	-0.006125	1.212617
33.396923	339.369835	4.496435	-0.006228	1.222712
34.124200	347.934982	4.501440	-0.006369	1.232744
34.883248	356.449873	4.506445	-0.006515	1.242643
35.290749	365.026042	4.511450	-0.006597	1.252466
36.200588	373.501625	4.516454	-0.006771	1.262194
36.586855	382.056945	4.521459	-0.006849	1.271838
37.154840	390.560283	4.526464	-0.006960	1.281386
37.927447	399.024995	4.531469	-0.007109	1.290858
38.442777	407.514039	4.536474	-0.007211	1.300240
39.338833	415.982944	4.541478	-0.007383	1.309602
39.751346	424.540844	4.546483	-0.007465	1.318906
40.450072	432.930380	4.551488	-0.007601	1.328015
41.090222	441.334080	4.556493	-0.007725	1.337067
41.619139	449.733210	4.561498	-0.007829	1.346034
42.168632	458.152059	4.566502	-0.007937	1.354965
42.836803	466.507146	4.571507	-0.008066	1.363792
43.536095	474.884796	4.576512	-0.008202	1.372590
44.014129	483.266974	4.581517	-0.008296	1.381299
44.438088	491.676795	4.586522	-0.008381	1.389972
45.028761	500.034891	4.591526	-0.008496	1.398567
45.174199	508.420395	4.596531	-0.008528	1.407062
45.953221	516.730228	4.601536	-0.008679	1.415535
46.277191	525.082812	4.606541	-0.008744	1.423926
46.868328	533.403725	4.611546	-0.008860	1.432279
47.323133	541.724560	4.616550	-0.008950	1.440562
47.758518	550.038785	4.621555	-0.009036	1.448787
48.441843	558.336575	4.626560	-0.009169	1.456989
49.269483	566.582407	4.631565	-0.009328	1.465118
49.807879	574.934357	4.636570	-0.009433	1.473258
50.199530	583.252411	4.641574	-0.009512	1.481298
50.413786	591.567019	4.646579	-0.009557	1.489264
51.151769	599.814841	4.651584	-0.009700	1.497204
51.691157	608.064113	4.656589	-0.009805	1.505074
52.048290	616.369200	4.661594	-0.009877	1.512926
52.628090	624.606811	4.666598	-0.009990	1.520709
52.979609	632.870995	4.671603	-0.010061	1.528442
53.525227	641.124517	4.676608	-0.010168	1.536156
53.653863	649.414431	4.681613	-0.010197	1.543801
54.174985	657.668740	4.686618	-0.010299	1.551435
54.780603	665.888888	4.691622	-0.010417	1.559013
55.214405	674.095085	4.696627	-0.010503	1.566516
55.627199	682.361069	4.701632	-0.010585	1.574034
56.224961	690.540586	4.706637	-0.010702	1.581465
56.648213	698.788486	4.711642	-0.010786	1.588897
57.168504	707.013866	4.716646	-0.010888	1.596288
57.827683	715.183797	4.721651	-0.011016	1.603616
58.199338	723.434131	4.726656	-0.011091	1.610940
58.468101	731.675855	4.731661	-0.011146	1.618209
59.041682	739.854450	4.736666	-0.011258	1.625433
59.606115	748.111167	4.741670	-0.011368	1.632691
59.991275	756.303818	4.746675	-0.011445	1.639837
60.638133	764.468270	4.751680	-0.011571	1.646963
60.888398	772.702101	4.756685	-0.011623	1.654064
61.533189	780.843357	4.761690	-0.011748	1.661108
61.853451	789.061539	4.766694	-0.011813	1.668145
62.458950	797.229503	4.771699	-0.011931	1.675147
62.892104	805.417748	4.776704	-0.012017	1.682114
62.992670	813.648216	4.781709	-0.012041	1.689044
63.350283	821.843416	4.786714	-0.012112	1.695950
64.184628	829.954024	4.791718	-0.012273	1.702820
64.160672	838.205529	4.796723	-0.012274	1.709666
64.689337	846.378150	4.801728	-0.012377	1.716492
64.995792	854.544190	4.806733	-0.012440	1.723257
65.708848	862.651357	4.811738	-0.012577	1.729999
66.169988	870.840572	4.816742	-0.012669	1.736749
66.507448	879.001207	4.821747	-0.012737	1.743434
67.024846	887.168862	4.826752	-0.012838	1.750122
67.370823	895.339917	4.831757	-0.012908	1.756766
67.787839	903.486105	4.836762	-0.012991	1.763373
68.197845	911.656194	4.841766	-0.013072	1.769974
68.495158	919.828354	4.846771	-0.013133	1.776537
68.958771	927.980053	4.851776	-0.013224	1.783081
69.325952	936.143621	4.856781	-0.013298	1.789598
69.948192	944.314220	4.861786	-0.013419	1.796128
70.222095	952.467202	4.866790	-0.013475	1.802579
70.579239	960.587753	4.871795	-0.013547	1.808990
71.064194	968.733750	4.876800	-0.013642	1.815414
71.462266	976.860243	4.881805	-0.013721	1.821790
71.822533	985.008941	4.886810	-0.013794	1.828156
72.483356	993.131264	4.891814	-0.013922	1.834515
72.932864	1001.237984	4.896819	-0.014011	1.840815
73.165575	1009.410472	4.901824	-0.014059	1.847119
73.508047	1017.574069	4.906829	-0.014128	1.853407
73.855521	1025.714332	4.911834	-0.014198	1.859656
74.091241	1033.870612	4.916838	-0.014247	1.865883
74.368831	1042.034989	4.921843	-0.014304	1.872101
74.891600	1050.148401	4.926848	-0.014407	1.878288
75.005895	1058.285000	4.931853	-0.014433	1.884425
75.460273	1066.396526	4.936858	-0.014523	1.890562
76.003860	1074.523800	4.941862	-0.014629	1.896700
76.096522	1082.663878	4.946867	-0.014652	1.902778
76.429982	1090.799710	4.951872	-0.014719	1.908860
76.757567	1098.935465	4.956877	-0.014785	1.914922
77.270476	1107.015727	4.961882	-0.014886	1.920944
77.661545	1115.120022	4.966886	-0.014964	1.926951
77.942526	1123.253138	4.971891	-0.015021	1.932949
78.618426	1131.341651	4.976896	-0.015152	1.938939
78.917122	1139.452658	4.981901	-0.015213	1.944885
79.396015	1147.594195	4.986906	-0.015307	1.950855
79.837503	1155.744922	4.991910	-0.015395	1.956809
80.149781	1163.820983	4.996915	-0.015458	1.962677
80.568378	1171.925135	5.001920	-0.015541	1.968560
81.028945	1180.038710	5.006925	-0.015632	1.974435
81.286063	1188.146505	5.011930	-0.015685	1.980268
81.615525	1196.264160	5.016934	-0.015752	1.986098
82.112219	1204.345948	5.021939	-0.015849	1.991903
82.981469	1212.408297	5.026944	-0.016016	1.997716
83.201079	1220.530714	5.031949	-0.016062	2.003486
83.375530	1228.675244	5.036954	-0.016100	2.009251
83.848387	1236.782069	5.041958	-0.016193	2.015004
83.935380	1244.906424	5.046963	-0.016215	2.020713
84.395982	1253.004300	5.051968	-0.016305	2.026425
84.779484	1261.122442	5.056973	-0.016382	2.032128
85.157001	1269.217407	5.061978	-0.016458	2.037797
85.488011	1277.315937	5.066982	-0.016524	2.043449
85.794095	1285.410099	5.071987	-0.016586	2.049079
86.169474	1293.526599	5.076992	-0.016662	2.054716
86.412624	1301.622356	5.081997	-0.016712	2.060311
86.592318	1309.732516	5.087002	-0.016751	2.065893
87.014405	1317.844464	5.092006	-0.016834	2.071486
87.170962	1325.947765	5.097011	-0.016869	2.077031
87.719333	1334.012602	5.102016	-0.016976	2.082574
88.307757	1342.073054	5.107021	-0.017091	2.088103
88.712209	1350.180444	5.112026	-0.017171	2.093632
88.874784	1358.321517	5.117030	-0.017206	2.099144
89.227804	1366.379729	5.122035	-0.017277	2.104605
89.800405	1374.475576	5.127040	-0.017389	2.110098
89.986292	1382.653493	5.132045	-0.017429	2.115594
90.094332	1390.730258	5.137050	-0.017454	2.121001
90.805081	1398.746088	5.142054	-0.017592	2.126412
91.172040	1406.818934	5.147059	-0.017665	2.131813
91.363221	1414.945810	5.152064	-0.017706	2.137220
91.755194	1423.003186	5.157069	-0.017784	2.142586
92.199090	1431.068898	5.162074	-0.017872	2.147950
92.590722	1439.197506	5.167078	-0.017950	2.153336
92.592700	1447.297913	5.172083	-0.017955	2.158653
93.107555	1455.349923	5.177088	-0.018056	2.163974
93.449639	1463.443172	5.182093	-0.018125	2.169292
93.766782	1471.538273	5.187098	-0.018189	2.174596
93.840707	1479.659327	5.192102	-0.018208	2.179882
94.214428	1487.710632	5.197107	-0.018283	2.185137
94.544862	1495.818424	5.202112	-0.018350	2.190412
94.731844	1503.938218	5.207117	-0.018390	2.195669
95.016647	1511.980293	5.212122	-0.018448	2.200872
95.414798	1520.048502	5.217126	-0.018527	2.206090
95.698609	1528.125151	5.222131	-0.018585	2.211290
96.160531	1536.197931	5.227136	-0.018676	2.216492
96.619711	1544.245316	5.232141	-0.018767	2.221665
96.752424	1552.340653	5.237146	-0.018797	2.226827
97.033118	1560.446956	5.242150	-0.018854	2.231998
97.229031	1568.539465	5.247155	-0.018896	2.237140
97.424602	1576.613692	5.252160	-0.018937	2.242258
97.489149	1584.700752	5.257165	-0.018955	2.247362
98.040997	1592.752780	5.262170	-0.019062	2.252474
98.311792	1600.848660	5.267174	-0.019118	2.257578
98.432078	1608.920324	5.272179	-0.019146	2.262642
98.766308	1617.011761	5.277184	-0.019213	2.267726
99.044665	1625.153663	5.282189	-0.019270	2.272825
99.064925	1633.229142	5.287194	-0.019279	2.277848
99.469044	1641.252073	5.292198	-0.019359	2.282861
99.683953	1649.308180	5.297203	-0.019404	2.287868
100.044523	1657.387577	5.302208	-0.019477	2.292890
100.171783	1665.468877	5.307213	-0.019505	2.297882
100.611323	1673.494981	5.312218	-0.019592	2.302856
101.070583	1681.557180	5.317222	-0.019683	2.307843
101.236455	1689.654619	5.322227	-0.019719	2.312816
101.571322	1697.710191	5.327232	-0.019787	2.317767
101.755498	1705.780232	5.332237	-0.019826	2.322703
102.052707	1713.827768	5.337242	-0.019886	2.327625
102.367174	1721.916450	5.342246	-0.019950	2.332563
102.714448	1729.969811	5.347251	-0.020020	2.337471
103.246878	1738.002283	5.352256	-0.020124	2.342372
103.511282	1746.088809	5.357261	-0.020179	2.347273
103.501924	1754.227934	5.362266	-0.020182	2.352173
103.922112	1762.279933	5.367270	-0.020265	2.357045
104.060452	1770.326218	5.372275	-0.020296	2.361881
104.299899	1778.396619	5.377280	-0.020346	2.366730
104.506881	1786.487064	5.382285	-0.020390	2.371578
104.792360	1794.525192	5.387290	-0.020448	2.376391
105.317602	1802.569968	5.392294	-0.020551	2.381217
105.603730	1810.615295	5.397299	-0.020609	2.386015
106.066236	1818.695092	5.402304	-0.020701	2.390838
106.290884	1826.790793	5.407309	-0.020748	2.395641
106.632087	1834.817425	5.412314	-0.020816	2.400403
106.946495	1842.887686	5.417318	-0.020880	2.405179
107.026669	1850.961760	5.422323	-0.020900	2.409930
107.360103	1859.056284	5.427328	-0.020967	2.414703
107.785580	1867.079023	5.432333	-0.021051	2.419432
108.003774	1875.141723	5.437338	-0.021097	2.424158
108.371874	1883.208526	5.442342	-0.021171	2.428889
108.819989	1891.339014	5.447347	-0.021260	2.433654
109.181431	1899.363711	5.452352	-0.021332	2.438342
109.507746	1907.394701	5.457357	-0.021398	2.443022
109.547633	1915.478158	5.462362	-0.021410	2.447701
109.954229	1923.521399	5.467366	-0.021491	2.452376
110.131654	1931.598369	5.472371	-0.021529	2.457043
110.456210	1939.637607	5.477376	-0.021595	2.461692
110.902517	1947.676617	5.482381	-0.021683	2.466340
110.960898	1955.760990	5.487386	-0.021699	2.470977
111.472301	1963.828064	5.492390	-0.021800	2.475629
111.658731	1971.868078	5.497395	-0.021839	2.480232
111.801116	1979.941219	5.502400	-0.021871	2.484842
112.001927	1988.007863	5.507405	-0.021914	2.489445
112.307598	1996.070210	5.512410	-0.021976	2.494044
112.488908	2004.148834	5.517414	-0.022014	2.498635
112.892705	2012.166470	5.522419	-0.022095	2.503199
113.379232	2020.201896	5.527424	-0.022190	2.507771
113.432967	2028.329922	5.532429	-0.022206	2.512355
113.716260	2036.371384	5.537434	-0.022264	2.516898
113.993290	2044.431706	5.542438	-0.022320	2.521444
114.126567	2052.459386	5.547443	-0.022350	2.525952
114.386928	2060.536905	5.552448	-0.022404	2.530490
114.884469	2068.575009	5.557453	-0.022502	2.535014
115.173452	2076.581242	5.562458	-0.022560	2.539498
115.611037	2084.638478	5.567462	-0.022647	2.544012
115.860414	2092.688111	5.572467	-0.022699	2.548501
115.826700	2100.813688	5.577472	-0.022698	2.553004
116.277861	2108.846961	5.582477	-0.022787	2.557482
116.583876	2116.867448	5.587482	-0.022849	2.561935
116.961028	2124.915187	5.592486	-0.022924	2.566400
117.098851	2132.987522	5.597491	-0.022955	2.570854
117.413693	2141.055056	5.602496	-0.023019	2.575310
117.603192	2149.110675	5.607501	-0.023059	2.579743
117.780378	2157.157007	5.612506	-0.023097	2.584163
118.280663	2165.206422	5.617510	-0.023195	2.588598
118.640044	2173.389495	5.622515	-0.023268	2.593090
118.980204	2181.452338	5.627520	-0.023336	2.597506
119.342306	2189.439932	5.632525	-0.023409	2.601876
119.690625	2197.441459	5.637530	-0.023478	2.606245
120.005294	2205.487617	5.642534	-0.023542	2.610629
120.161544	2213.546106	5.647539	-0.023576	2.615001
120.448867	2221.573589	5.652544	-0.023635	2.619357
120.696469	2229.606214	5.657549	-0.023686	2.623707
120.868998	2237.658126	5.662554	-0.023723	2.628055
121.346222	2245.707660	5.667558	-0.023817	2.632414
121.555126	2253.763737	5.672563	-0.023861	2.636752
121.565126	2261.828830	5.677568	-0.023868	2.641074
122.027781	2269.845396	5.682573	-0.023960	2.645393
122.465271	2277.862346	5.687578	-0.024046	2.649704
122.663918	2285.970800	5.692582	-0.024088	2.654041
122.660927	2294.027795	5.697587	-0.024093	2.658330
122.987942	2302.069861	5.702592	-0.024159	2.662625
123.046913	2310.129526	5.707597	-0.024175	2.666906
123.232637	2318.191475	5.712602	-0.024215	2.671189
123.544182	2326.286044	5.717606	-0.024278	2.675490
123.629390	2334.278698	5.722611	-0.024299	2.679717
123.998079	2342.292951	5.727616	-0.024373	2.683966
124.558109	2350.329635	5.732621	-0.024482	2.688232
124.806608	2358.375416	5.737626	-0.024533	2.692476
125.178489	2366.450732	5.742630	-0.024608	2.696737
125.260839	2374.492779	5.747635	-0.024628	2.700956
125.631973	2382.527094	5.752640	-0.024703	2.705182
125.997925	2390.571227	5.757645	-0.024776	2.709406
126.064319	2398.665804	5.762650	-0.024793	2.713631
126.333895	2406.707942	5.767654	-0.024849	2.717834
126.745278	2414.687468	5.772659	-0.024930	2.722008
127.064891	2422.730149	5.777664	-0.024995	2.726202
127.267169	2430.785499	5.782669	-0.025038	2.730389
127.493746	2438.859510	5.787674	-0.025085	2.734581
127.853420	2446.893374	5.792678	-0.025157	2.738753
128.128924	2454.914537	5.797683	-0.025214	2.742908
128.341265	2462.976722	5.802688	-0.025258	2.747073
128.770826	2471.039616	5.807693	-0.025343	2.751245
128.941460	2479.154024	5.812698	-0.025380	2.755422
129.363937	2487.148855	5.817702	-0.025464	2.759547
129.743276	2495.148143	5.822707	-0.025540	2.763665
129.945859	2503.198637	5.827712	-0.025583	2.767792
130.140110	2511.264694	5.832717	-0.025624	2.771921
130.312216	2519.309925	5.837722	-0.025661	2.776031
130.650123	2527.342936	5.842726	-0.025729	2.780139
130.844757	2535.359208	5.847731	-0.025770	2.784224
130.948726	2543.425617	5.852736	-0.025795	2.788323
131.525696	2551.465109	5.857741	-0.025907	2.792430
131.652065	2559.516472	5.862746	-0.025936	2.796510
131.726820	2567.580077	5.867750	-0.025955	2.800588
132.128318	2575.558297	5.872755	-0.026035	2.804635
132.335258	2583.617840	5.877760	-0.026079	2.808707
132.641250	2591.685879	5.882765	-0.026141	2.812782
133.015431	2599.710685	5.887770	-0.026216	2.816834
133.339131	2607.753050	5.892774	-0.026281	2.820886
133.478636	2615.786451	5.897779	-0.026312	2.824917
133.705300	2623.839568	5.902784	-0.026359	2.828956
134.058866	2631.926768	5.907789	-0.026430	2.833015
134.265917	2639.950973	5.912794	-0.026474	2.837027
134.526519	2647.989357	5.917798	-0.026528	2.841045
134.784785	2655.984237	5.922803	-0.026581	2.845034
134.931031	2664.049117	5.927808	-0.026613	2.849047
135.341942	2672.096147	5.932813	-0.026695	2.853059
135.367921	2680.158451	5.937818	-0.026705	2.857052
135.862997	2688.174754	5.942822	-0.026802	2.861043
135.889700	2696.202078	5.947827	-0.026812	2.865008
136.258231	2704.250304	5.952832	-0.026886	2.868996
136.696266	2712.324989	5.957837	-0.026973	2.872996
136.897303	2720.357002	5.962842	-0.027015	2.876956
136.974971	2728.422891	5.967846	-0.027035	2.880920
137.299237	2736.397243	5.972851	-0.027100	2.884848
137.624569	2744.437399	5.977856	-0.027166	2.888802
137.946944	2752.499309	5.982861	-0.027231	2.892761
138.168877	2760.549040	5.987866	-0.027277	2.896704
138.300050	2768.609027	5.992870	-0.027307	2.900641
138.485685	2776.621412	5.997875	-0.027347	2.904552
138.797879	2784.657718	6.002880	-0.027410	2.908477
138.991030	2792.772210	6.007885	-0.027451	2.912428
139.278624	2800.801123	6.012890	-0.027510	2.916337
139.398267	2808.831673	6.017894	-0.027537	2.920233
139.470065	2816.842090	6.022899	-0.027556	2.924111
139.869938	2824.842816	6.027904	-0.027635	2.927996
140.119069	2832.895464	6.032909	-0.027687	2.931894
140.298125	2840.938721	6.037914	-0.027725	2.935778
140.585001	2848.951778	6.042918	-0.027784	2.939648
141.019841	2856.958833	6.047923	-0.027870	2.943518
141.024185	2865.034410	6.052928	-0.027876	2.947393
141.358710	2873.082931	6.057933	-0.027943	2.951267
141.541086	2881.135804	6.062938	-0.027982	2.955130
141.654348	2889.155786	6.067942	-0.028008	2.958969
141.930983	2897.160809	6.072947	-0.028065	2.962804
142.173609	2905.215401	6.077952	-0.028115	2.966656
142.303359	2913.292704	6.082957	-0.028145	2.970508
142.290849	2921.329435	6.087962	-0.028147	2.974328
142.599126	2929.358664	6.092966	-0.028210	2.978156
142.899266	2937.365665	6.097971	-0.028271	2.981969
142.938482	2945.414819	6.102976	-0.028283	2.985783
143.438167	2953.424030	6.107981	-0.028381	2.989596
143.510673	2961.524106	6.112986	-0.028400	2.993426
143.930351	2969.551488	6.117990	-0.028483	2.997235
144.147991	2977.570219	6.122995	-0.028529	3.001024
144.354149	2985.561251	6.128000	-0.028572	3.004795
144.736246	2993.611039	6.133005	-0.028649	3.008597
145.029347	3001.641972	6.138010	-0.028708	3.012381
145.348078	3009.693135	6.143014	-0.028773	3.016171
145.486061	3017.704806	6.148019	-0.028804	3.019929
145.782666	3025.734003	6.153024	-0.028864	3.023698
145.995843	3033.789443	6.158029	-0.028909	3.027471
146.188563	3041.828381	6.163034	-0.028950	3.031230
146.361600	3049.896215	6.168038	-0.028987	3.034997
146.691567	3057.892093	6.173043	-0.029054	3.038734
147.009923	3065.904570	6.178048	-0.029118	3.042472
147.617576	3073.938903	6.183053	-0.029236	3.046231
147.581159	3081.987253	6.188058	-0.029235	3.049960
147.969518	3090.051631	6.193062	-0.029312	3.053712
148.146074	3098.079675	6.198067	-0.029350	3.057433
148.392507	3106.120573	6.203072	-0.029401	3.061159
148.563216	3114.160870	6.208077	-0.029438	3.064876
148.646805	3122.204331	6.213082	-0.029459	3.068586
148.806039	3130.304846	6.218086	-0.029493	3.072321
149.181222	3138.368857	6.223091	-0.029568	3.076045
149.493295	3146.304988	6.228096	-0.029632	3.079702
149.895344	3154.324033	6.233101	-0.029712	3.083398
150.326313	3162.310420	6.238106	-0.029797	3.087075
150.728141	3170.370283	6.243110	-0.029877	3.090780
151.104363	3178.414578	6.248115	-0.029952	3.094473
151.027645	3186.469074	6.253120	-0.029943	3.098145
151.386951	3194.484504	6.258125	-0.030015	3.101814
151.668880	3202.477572	6.263130	-0.030072	3.105466
151.774120	3210.532911	6.268134	-0.030097	3.109133
151.933076	3218.611719	6.273139	-0.030132	3.112809
152.167325	3226.649276	6.278144	-0.030181	3.116466
152.442866	3234.648855	6.283149	-0.030237	3.120103
152.531298	3242.663370	6.288154	-0.030259	3.123733
152.878808	3250.718265	6.293158	-0.030328	3.127390
153.108740	3258.761876	6.298163	-0.030376	3.131032
153.125615	3266.797899	6.303168	-0.030385	3.134656
153.683805	3274.813509	6.308173	-0.030494	3.138292
153.806450	3282.839850	6.313178	-0.030522	3.141908
154.006094	3290.876991	6.318182	-0.030564	3.145529
154.164195	3298.919215	6.323187	-0.030598	3.149146
154.457040	3306.959696	6.328192	-0.030658	3.152763
154.845176	3315.020505	6.333197	-0.030735	3.156390
154.670931	3322.997465	6.338202	-0.030708	3.159951
155.123578	3331.002859	6.343206	-0.030797	3.163547
155.612306	3339.025298	6.348211	-0.030894	3.167149
155.998386	3347.063546	6.353216	-0.030971	3.170749
156.111550	3355.145191	6.358221	-0.030997	3.174352
156.259498	3363.154070	6.363226	-0.031029	3.177921
156.481636	3371.201461	6.368230	-0.031076	3.181506
156.540303	3379.220937	6.373235	-0.031092	3.185067
156.828760	3387.257724	6.378240	-0.031151	3.188641
157.163052	3395.323992	6.383245	-0.031218	3.192227
157.175111	3403.373728	6.388250	-0.031226	3.195788
157.596489	3411.327034	6.393254	-0.031309	3.199319
157.995434	3419.357304	6.398259	-0.031388	3.202879
158.109965	3427.415167	6.403264	-0.031415	3.206436
158.057770	3435.458079	6.408269	-0.031410	3.209975
158.423215	3443.482503	6.413274	-0.031483	3.213519
158.726520	3451.539602	6.418278	-0.031545	3.217072
158.844376	3459.556996	6.423283	-0.031572	3.220595
159.095423	3467.552213	6.428288	-0.031624	3.224110
159.382552	3475.609264	6.433293	-0.031683	3.227650
159.512483	3483.653571	6.438298	-0.031712	3.231173
159.677914	3491.753467	6.443302	-0.031748	3.234719
159.836300	3499.744182	6.448307	-0.031782	3.238213
160.013281	3507.725405	6.453312	-0.031820	3.241700
160.223364	3515.755284	6.458317	-0.031865	3.245205
160.631574	3523.724658	6.463322	-0.031946	3.248688
160.912276	3531.791469	6.468326	-0.032003	3.252205
161.036214	3539.863595	6.473331	-0.032031	3.255714
161.055942	3547.889233	6.478336	-0.032040	3.259194
161.563083	3555.909080	6.483341	-0.032140	3.262688
161.666356	3563.919849	6.488346	-0.032164	3.266158
161.917020	3571.942364	6.493350	-0.032216	3.269636
162.200872	3580.011042	6.498355	-0.032274	3.273130
162.405415	3588.044272	6.503360	-0.032317	3.276603
162.562923	3596.057770	6.508365	-0.032351	3.280062
162.948377	3604.031601	6.513370	-0.032428	3.283508
163.274540	3612.073850	6.518374	-0.032494	3.286978
163.286488	3620.136345	6.523379	-0.032501	3.290441
163.466304	3628.183517	6.528384	-0.032540	3.293900
163.772400	3636.206775	6.533389	-0.032602	3.297351
163.705029	3644.244295	6.538394	-0.032595	3.300789
163.881370	3652.239916	6.543398	-0.032633	3.304215
164.066974	3660.298670	6.548403	-0.032672	3.307665
164.438315	3668.315015	6.553408	-0.032747	3.311100
164.695873	3676.385137	6.558413	-0.032800	3.314550
164.750351	3684.351223	6.563418	-0.032815	3.317945
165.122708	3692.376710	6.568422	-0.032889	3.321373
165.157315	3700.413990	6.573427	-0.032901	3.324790
165.251851	3708.432218	6.578432	-0.032924	3.328198
165.699735	3716.462319	6.583437	-0.033012	3.331620
165.798482	3724.497559	6.588442	-0.033036	3.335028
165.952455	3732.548055	6.593446	-0.033069	3.338441
166.266492	3740.596610	6.598451	-0.033133	3.341855
166.425109	3748.562798	6.603456	-0.033168	3.345226
166.606918	3756.612819	6.608461	-0.033207	3.348629
166.566160	3764.677799	6.613466	-0.033204	3.352027
166.964943	3772.705555	6.618470	-0.033283	3.355422
167.114866	3780.726707	6.623475	-0.033316	3.358802
167.269256	3788.740022	6.628480	-0.033350	3.362175
167.867031	3796.748713	6.633485	-0.033467	3.365558
168.256336	3804.744874	6.638490	-0.033544	3.368926
168.436179	3812.829001	6.643494	-0.033583	3.372319
168.797164	3820.870103	6.648499	-0.033655	3.375697
169.145656	3828.820393	6.653504	-0.033725	3.379034
169.385271	3836.900869	6.658509	-0.033775	3.382417
169.427994	3844.909658	6.663514	-0.033788	3.385761
169.631395	3852.981007	6.668518	-0.033831	3.389132
169.613570	3861.076887	6.673523	-0.033833	3.392503
169.812779	3869.118276	6.678528	-0.033875	3.395856
170.008811	3877.090571	6.683533	-0.033917	3.399176
170.231716	3885.068510	6.688538	-0.033963	3.402496
170.443595	3893.079370	6.693542	-0.034008	3.405826
170.617753	3901.114886	6.698547	-0.034045	3.409162
170.841297	3909.157276	6.703552	-0.034092	3.412499
170.990315	3917.204765	6.708557	-0.034125	3.415833
171.301879	3925.177956	6.713562	-0.034188	3.419138
171.759839	3933.188555	6.718566	-0.034278	3.422460
171.933141	3941.225287	6.723571	-0.034316	3.425780
172.046377	3949.252847	6.728576	-0.034342	3.429091
172.286121	3957.315050	6.733581	-0.034392	3.432417
172.495126	3965.338326	6.738586	-0.034436	3.435723
172.731982	3973.361080	6.743590	-0.034485	3.439026
172.992231	3981.380630	6.748595	-0.034539	3.442326
173.040469	3989.389396	6.753600	-0.034553	3.445611
173.225299	3997.459599	6.758605	-0.034592	3.448922
173.228525	4005.517966	6.763610	-0.034598	3.452220
173.455342	4013.542349	6.768614	-0.034645	3.455507
173.673778	4021.554510	6.773619	-0.034691	3.458787
173.792902	4029.583876	6.778624	-0.034718	3.462067
174.174780	4037.579983	6.783629	-0.034794	3.465339
174.413452	4045.596789	6.788634	-0.034844	3.468611
174.579716	4053.664665	6.793638	-0.034880	3.471899
174.811011	4061.696688	6.798643	-0.034928	3.475171
175.078911	4069.667346	6.803648	-0.034983	3.478416
175.200776	4077.729486	6.808653	-0.035011	3.481691
175.427128	4085.676993	6.813658	-0.035058	3.484920
175.692725	4093.733027	6.818662	-0.035113	3.488190
175.919091	4101.777438	6.823667	-0.035160	3.491452
175.782533	4109.821548	6.828672	-0.035140	3.494699
176.009939	4117.860929	6.833677	-0.035187	3.497952
176.379469	4125.841100	6.838682	-0.035261	3.501183
176.574179	4133.835416	6.843686	-0.035303	3.504411
176.748332	4141.879903	6.848691	-0.035340	3.507656
177.120042	4149.895703	6.853696	-0.035414	3.510892
177.271753	4157.970999	6.858701	-0.035448	3.514142
177.327227	4165.985792	6.863706	-0.035463	3.517362
177.507304	4174.006975	6.868710	-0.035502	3.520586
177.831284	4182.006671	6.873715	-0.035567	3.523802
177.790302	4190.034647	6.878720	-0.035565	3.527016
177.990325	4198.090634	6.883725	-0.035607	3.530245
178.369249	4206.114733	6.888730	-0.035683	3.533464
178.667750	4214.156327	6.893734	-0.035743	3.536684
178.961288	4222.148621	6.898739	-0.035803	3.539881
179.229320	4230.137664	6.903744	-0.035858	3.543074
179.389036	4238.238645	6.908749	-0.035893	3.546305
179.425921	4246.261308	6.913754	-0.035905	3.549498
179.617297	4254.370035	6.918758	-0.035946	3.552727
180.023789	4262.403359	6.923763	-0.036027	3.555930
180.123279	4270.353584	6.928768	-0.036050	3.559087
180.277789	4278.347810	6.933773	-0.036084	3.562261
180.518431	4286.355491	6.938778	-0.036134	3.565440
180.553688	4294.375319	6.943782	-0.036146	3.568615
180.847481	4302.422007	6.948787	-0.036205	3.571805
180.919600	4310.441685	6.953792	-0.036224	3.574975
181.487502	4318.437001	6.958797	-0.036335	3.578147
181.508818	4326.465297	6.963802	-0.036344	3.581313
181.607594	4334.473672	6.968806	-0.036367	3.584471
181.962428	4342.520570	6.973811	-0.036439	3.587649
182.052159	4350.538361	6.978816	-0.036460	3.590804
182.393819	4358.599124	6.983821	-0.036529	3.593981
182.450633	4366.612897	6.988826	-0.036545	3.597129
182.724237	4374.596658	6.993830	-0.036601	3.600268
182.791064	4382.623840	6.998835	-0.036618	3.603416
182.812578	4390.651741	7.003840	-0.036628	3.606560
183.246664	4398.638124	7.008845	-0.036713	3.609696
183.115384	4406.712557	7.013850	-0.036694	3.612848
183.366746	4414.741299	7.018854	-0.036746	3.615991
183.743540	4422.749074	7.023859	-0.036821	3.619125
183.779522	4430.763935	7.028864	-0.036833	3.622251
184.128485	4438.807865	7.033869	-0.036903	3.625393
184.242393	4446.830455	7.038874	-0.036930	3.628519
184.370230	4454.874309	7.043878	-0.036958	3.631650
184.529136	4462.944713	7.048883	-0.036993	3.634789
184.952204	4470.924163	7.053888	-0.037077	3.637898
185.158460	4478.965919	7.058893	-0.037121	3.641022
185.249448	4486.927525	7.063898	-0.037143	3.644109
185.409493	4494.953295	7.068902	-0.037177	3.647221
185.603198	4503.021635	7.073907	-0.037219	3.650347
185.903816	4511.030670	7.078912	-0.037280	3.653450
185.958163	4519.105531	7.083917	-0.037295	3.656569
186.126611	4527.069454	7.088922	-0.037331	3.659647
186.381869	4535.107997	7.093926	-0.037384	3.662752
186.492802	4543.130817	7.098931	-0.037410	3.665845
186.495275	4551.149936	7.103936	-0.037415	3.668931
187.071064	4559.185962	7.108941	-0.037528	3.672036
187.304872	4567.204039	7.113946	-0.037576	3.675122
187.334260	4575.205219	7.118950	-0.037587	3.678194
187.933524	4583.233716	7.123955	-0.037704	3.681289
188.104009	4591.184479	7.128960	-0.037740	3.684340
188.453618	4599.276047	7.133965	-0.037811	3.687447
188.603914	4607.291447	7.138970	-0.037844	3.690517
188.860375	4615.334376	7.143974	-0.037897	3.693598
189.071968	4623.411626	7.148979	-0.037941	3.696688
189.129465	4631.360966	7.153984	-0.037957	3.699723
189.372442	4639.394029	7.158989	-0.038007	3.702792
189.568400	4647.395124	7.163994	-0.038049	3.705845
189.661971	4655.430897	7.168998	-0.038071	3.708906
190.068634	4663.508917	7.174003	-0.038152	3.711988
190.044913	4671.571498	7.179008	-0.038153	3.715052
190.334048	4679.553137	7.184013	-0.038212	3.718089
190.546201	4687.519213	7.189018	-0.038256	3.721117
190.752224	4695.503802	7.194022	-0.038300	3.724149
190.987413	4703.550032	7.199027	-0.038349	3.727202
191.031238	4711.558198	7.204032	-0.038362	3.730234
191.313639	4719.599901	7.209037	-0.038420	3.733281
191.519972	4727.672127	7.214042	-0.038463	3.736336
191.637320	4735.647462	7.219046	-0.038490	3.739350
191.898240	4743.662496	7.224051	-0.038544	3.742380
191.988896	4751.659178	7.229056	-0.038566	3.745396
192.358250	4759.700515	7.234061	-0.038640	3.748433
192.425229	4767.766535	7.239066	-0.038657	3.751470
192.576141	4775.793216	7.244070	-0.038691	3.754491
192.673952	4783.871288	7.249075	-0.038714	3.757528
192.866268	4791.793699	7.254080	-0.038755	3.760507
193.150402	4799.849234	7.259085	-0.038813	3.763535
193.201128	4807.880688	7.264090	-0.038827	3.766546
193.347562	4815.869384	7.269094	-0.038860	3.769541
193.512110	4823.941027	7.274099	-0.038896	3.772565
193.819593	4831.938709	7.279104	-0.038958	3.775562
193.957774	4839.987407	7.284109	-0.038989	3.778572
194.147135	4848.001852	7.289114	-0.039029	3.781568
194.154186	4855.985132	7.294118	-0.039035	3.784545
194.228886	4864.079601	7.299123	-0.039055	3.787564
194.353385	4872.047594	7.304128	-0.039083	3.790534
194.550634	4880.114094	7.309133	-0.039125	3.793540
194.770779	4888.124404	7.314138	-0.039171	3.796523
194.977577	4896.104915	7.319142	-0.039214	3.799492
194.991071	4904.156164	7.324147	-0.039222	3.802481
195.234717	4912.151404	7.329152	-0.039272	3.805452
195.471516	4920.149193	7.334157	-0.039322	3.808421
195.692409	4928.193054	7.339162	-0.039368	3.811405
195.911418	4936.172535	7.344166	-0.039414	3.814362
195.907715	4944.279337	7.349171	-0.039418	3.817360
196.055789	4952.229898	7.354176	-0.039451	3.820300
196.209275	4960.284478	7.359181	-0.039485	3.823277
196.538552	4968.279444	7.364186	-0.039551	3.826233
196.834517	4976.274174	7.369190	-0.039611	3.829187
196.925592	4984.368293	7.374195	-0.039633	3.832170
197.191333	4992.349371	7.379200	-0.039688	3.835112
197.597564	5000.378857	7.384205	-0.039769	3.838074
197.544048	5008.428760	7.389210	-0.039764	3.841031
197.894431	5016.388994	7.394214	-0.039834	3.843961
198.197756	5024.462802	7.399219	-0.039896	3.846929
198.261385	5032.437945	7.404224	-0.039913	3.849854
198.408437	5040.516005	7.409229	-0.039945	3.852816
198.712056	5048.520854	7.414234	-0.040007	3.855752
198.641391	5056.522731	7.419238	-0.039999	3.858678
198.937240	5064.558337	7.424243	-0.040059	3.861620
199.197693	5072.534588	7.429248	-0.040112	3.864539
199.404705	5080.648286	7.434253	-0.040156	3.867504
199.336987	5088.683911	7.439258	-0.040149	3.870432
199.576690	5096.851210	7.444262	-0.040198	3.873413
200.065959	5104.861299	7.449267	-0.040295	3.876339
200.139391	5112.726645	7.454272	-0.040313	3.879202
200.303167	5120.760517	7.459277	-0.040349	3.882125
200.586510	5128.709010	7.464282	-0.040407	3.885018
200.841777	5136.737327	7.469286	-0.040459	3.887937
200.871493	5144.798407	7.474291	-0.040470	3.890862
201.025374	5152.815056	7.479296	-0.040504	3.893770
201.207787	5160.875937	7.484301	-0.040543	3.896693
201.190512	5168.844701	7.489306	-0.040545	3.899577
201.454865	5176.840903	7.494310	-0.040599	3.902473
201.756922	5184.854164	7.499315	-0.040660	3.905374
201.694035	5192.882956	7.504320	-0.040654	3.908272
201.826319	5200.924903	7.509325	-0.040684	3.911176
202.060330	5208.963316	7.514330	-0.040732	3.914079
201.934429	5216.982938	7.519334	-0.040714	3.916966
202.197729	5224.961629	7.524339	-0.040768	3.919843
202.569606	5232.952055	7.529344	-0.040842	3.922724
202.761131	5240.995903	7.534349	-0.040883	3.925619
202.676844	5249.008427	7.539354	-0.040873	3.928496
202.960647	5257.035227	7.544358	-0.040930	3.931382
203.311394	5265.093429	7.549363	-0.041001	3.934279
203.549236	5273.092787	7.554368	-0.041050	3.937150
203.833811	5281.078326	7.559373	-0.041108	3.940015
203.989471	5289.103250	7.564378	-0.041142	3.942890
204.342767	5297.118229	7.569382	-0.041213	3.945762
204.614861	5305.155437	7.574387	-0.041269	3.948639
204.768481	5313.175573	7.579392	-0.041303	3.951506
204.945819	5321.249461	7.584397	-0.041341	3.954390
205.079957	5329.263107	7.589402	-0.041371	3.957250
205.212293	5337.211704	7.594406	-0.041401	3.960084
205.713644	5345.246503	7.599411	-0.041499	3.962954
205.770970	5353.226159	7.604416	-0.041515	3.965794
205.781082	5361.274436	7.609421	-0.041522	3.968655
205.865940	5369.314424	7.614426	-0.041543	3.971513
205.988275	5377.332077	7.619430	-0.041571	3.974362
206.090955	5385.422494	7.624435	-0.041595	3.977234
206.164008	5393.362511	7.629440	-0.041614	3.980050
206.508704	5401.424171	7.634445	-0.041683	3.982911
206.719489	5409.395693	7.639450	-0.041727	3.985737
206.752923	5417.438595	7.644454	-0.041739	3.988583
207.015662	5425.476650	7.649459	-0.041793	3.991428
207.429922	5433.479980	7.654464	-0.041875	3.994262
207.576001	5441.543951	7.659469	-0.041907	3.997111
207.776802	5449.508536	7.664474	-0.041950	3.999924
208.054051	5457.536477	7.669478	-0.042006	4.002758
208.288848	5465.559741	7.674483	-0.042055	4.005588
208.354489	5473.581331	7.679488	-0.042073	4.008412
208.321396	5481.649453	7.684493	-0.042072	4.011249
208.523460	5489.676334	7.689498	-0.042114	4.014074
208.488897	5497.696377	7.694502	-0.042113	4.016890
208.877788	5505.698821	7.699507	-0.042190	4.019705
209.013557	5513.684380	7.704512	-0.042221	4.022508
209.087381	5521.718391	7.709517	-0.042240	4.025325
209.234802	5529.728099	7.714522	-0.042272	4.028132
209.434846	5537.770618	7.719526	-0.042315	4.030950
209.691776	5545.903898	7.724531	-0.042368	4.033799
209.623399	5553.873007	7.729536	-0.042360	4.036583
210.043316	5561.824827	7.734541	-0.042443	4.039367
210.291517	5569.843348	7.739546	-0.042495	4.042169
210.332846	5577.816357	7.744550	-0.042507	4.044950
210.634632	5585.873446	7.749555	-0.042569	4.047763
210.868520	5593.861125	7.754560	-0.042617	4.050548
211.178447	5601.901463	7.759565	-0.042680	4.053351
211.226964	5609.931492	7.764570	-0.042694	4.056145
211.633647	5617.880298	7.769574	-0.042775	4.058914
211.470357	5626.024659	7.774579	-0.042750	4.061740
211.553208	5633.926938	7.779584	-0.042770	4.064484
211.898103	5641.976919	7.784589	-0.042840	4.067281
211.919281	5649.977330	7.789594	-0.042849	4.070054
211.847112	5658.019465	7.794598	-0.042840	4.072839
212.350574	5666.079896	7.799603	-0.042939	4.075636
212.590346	5674.032994	7.804608	-0.042989	4.078390
212.967958	5682.035749	7.809613	-0.043064	4.081161
212.910650	5690.046070	7.814618	-0.043059	4.083927
213.311102	5698.076222	7.819622	-0.043138	4.086705
213.394352	5706.115475	7.824627	-0.043159	4.089479
213.310906	5714.175834	7.829632	-0.043149	4.092256
213.533330	5722.178920	7.834637	-0.043195	4.095016
213.628691	5730.212403	7.839642	-0.043218	4.097783
213.846646	5738.171269	7.844646	-0.043264	4.100524
214.007974	5746.245842	7.849651	-0.043299	4.103302
214.141072	5754.246136	7.854656	-0.043329	4.106052
214.434918	5762.240272	7.859661	-0.043388	4.108800
214.547715	5770.299550	7.864666	-0.043415	4.111566
214.910216	5778.333942	7.869670	-0.043487	4.114326
215.212201	5786.394387	7.874675	-0.043549	4.117091
215.206072	5794.329586	7.879680	-0.043552	4.119808
215.403320	5802.377485	7.884685	-0.043594	4.122564
215.388551	5810.326342	7.889690	-0.043597	4.125282
215.635494	5818.371366	7.894694	-0.043648	4.128034
216.007164	5826.413651	7.899699	-0.043722	4.130785
216.313665	5834.478471	7.904704	-0.043784	4.133540
216.389081	5842.514118	7.909709	-0.043803	4.136281
216.305892	5850.497601	7.914714	-0.043793	4.139001
216.652998	5858.536947	7.919718	-0.043863	4.141743
216.750507	5866.532836	7.924723	-0.043886	4.144465
216.870536	5874.550680	7.929728	-0.043913	4.147194
217.069095	5882.579368	7.934733	-0.043956	4.149925
217.395756	5890.621825	7.939738	-0.044021	4.152660
217.332542	5898.631766	7.944742	-0.044015	4.155378
217.456345	5906.637700	7.949747	-0.044043	4.158096
217.474121	5914.629543	7.954752	-0.044051	4.160805
217.635205	5922.646599	7.959757	-0.044086	4.163522
217.949478	5930.680361	7.964762	-0.044150	4.166246
217.976415	5938.674770	7.969766	-0.044160	4.168951
218.111362	5946.752968	7.974771	-0.044190	4.171683
218.091718	5954.776990	7.979776	-0.044192	4.174394
218.341337	5962.772306	7.984781	-0.044243	4.177097
218.399167	5970.787575	7.989786	-0.044259	4.179802
218.620903	5978.777678	7.994790	-0.044306	4.182499
218.885336	5986.799445	7.999795	-0.044360	4.185205
218.840352	5994.818014	8.004800	-0.044357	4.187905
219.226289	6002.818565	8.009805	-0.044434	4.190601
219.266075	6010.951604	8.014810	-0.044446	4.193337
219.454315	6018.953307	8.019814	-0.044486	4.196029
219.883663	6026.916333	8.024819	-0.044571	4.198708
219.760317	6034.913191	8.029824	-0.044554	4.201391
219.901772	6042.898455	8.034829	-0.044585	4.204071
220.203696	6050.964935	8.039834	-0.044646	4.206779
220.232862	6058.898822	8.044838	-0.044657	4.209437
220.532197	6067.001074	8.049843	-0.044718	4.212153
220.816749	6075.000866	8.054848	-0.044776	4.214833
220.898048	6083.017638	8.059853	-0.044796	4.217514
220.939017	6091.022075	8.064858	-0.044809	4.220189
221.155677	6099.017942	8.069862	-0.044854	4.222862
221.477106	6107.050477	8.074867	-0.044919	4.225546
221.456125	6115.059981	8.079872	-0.044920	4.228217
221.575983	6123.062920	8.084877	-0.044948	4.230886
221.799956	6131.132624	8.089882	-0.044995	4.233576
221.934516	6139.141664	8.094886	-0.045025	4.236243
222.124991	6147.148574	8.099891	-0.045065	4.238909
222.317797	6155.125786	8.104896	-0.045106	4.241563
222.533857	6163.135618	8.109901	-0.045152	4.244226
222.609394	6171.181811	8.114906	-0.045171	4.246899
222.558455	6179.180182	8.119910	-0.045166	4.249552
222.871067	6187.239356	8.124915	-0.045230	4.252228
222.922655	6195.271367	8.129920	-0.045244	4.254890
223.169946	6203.295532	8.134925	-0.045296	4.257550
223.243136	6211.301254	8.139930	-0.045314	4.260201
223.568049	6219.274045	8.144934	-0.045380	4.262841
223.690458	6227.348981	8.149939	-0.045408	4.265512
223.828606	6235.335980	8.154944	-0.045439	4.268152
224.090196	6243.384314	8.159949	-0.045492	4.270811
224.037591	6251.446966	8.164954	-0.045488	4.273471
224.013905	6259.480728	8.169958	-0.045489	4.276120
224.357003	6267.422810	8.174963	-0.045557	4.278741
224.386712	6275.470868	8.179968	-0.045568	4.281392
224.852049	6283.420813	8.184973	-0.045660	4.284012
224.922025	6291.506378	8.189978	-0.045678	4.286672
225.042397	6299.459891	8.194982	-0.045705	4.289288
225.030942	6307.539462	8.199987	-0.045708	4.291942
225.190319	6315.554194	8.204992	-0.045743	4.294575
225.480833	6323.602114	8.209997	-0.045802	4.297218
225.532181	6331.590447	8.215002	-0.045817	4.299838
225.558919	6339.596662	8.220006	-0.045827	4.302462
225.921882	6347.618819	8.225011	-0.045900	4.305093
225.938223	6355.638984	8.230016	-0.045908	4.307718
226.094431	6363.615899	8.235021	-0.045942	4.310328
226.156252	6371.718372	8.240026	-0.045959	4.312978
226.374211	6379.679829	8.245030	-0.046004	4.315581
226.619624	6387.679033	8.250035	-0.046055	4.318194
226.988530	6395.717707	8.255040	-0.046129	4.320820
227.202215	6403.702680	8.260045	-0.046174	4.323426
226.975601	6411.742641	8.265050	-0.046137	4.326045
227.031633	6419.710183	8.270054	-0.046152	4.328640
227.335324	6427.788386	8.275059	-0.046214	4.331272
227.561986	6435.808033	8.280064	-0.046261	4.333883
227.679098	6443.832093	8.285069	-0.046288	4.336492
227.870404	6451.811401	8.290074	-0.046329	4.339086
227.978462	6459.847338	8.295078	-0.046354	4.341697
228.278103	6467.802351	8.300083	-0.046415	4.344281
228.403560	6475.814951	8.305088	-0.046444	4.346880
228.562367	6483.857732	8.310093	-0.046478	4.349488
228.825004	6491.965955	8.315098	-0.046532	4.352117
229.043600	6500.000022	8.320102	-0.046578	4.354719
229.082339	6508.058028	8.325107	-0.046590	4.357327
229.319590	6515.956638	8.330112	-0.046640	4.359882
229.467193	6523.959341	8.335117	-0.046672	4.362470
229.484598	6531.937481	8.340122	-0.046681	4.365047
229.637811	6539.939023	8.345126	-0.046714	4.367630
229.942583	6548.015093	8.350131	-0.046776	4.370237
230.030599	6556.006239	8.355136	-0.046798	4.372814
230.098162	6564.062614	8.360141	-0.046815	4.375411
230.350484	6572.116522	8.365146	-0.046867	4.378006
230.472497	6580.065132	8.370150	-0.046895	4.380564
230.700391	6588.069935	8.375155	-0.046943	4.383140
230.805840	6596.095333	8.380160	-0.046967	4.385721
231.022457	6604.133265	8.385165	-0.047013	4.388304
231.179045	6612.180967	8.390170	-0.047047	4.390889
231.510750	6620.137023	8.395174	-0.047114	4.393444
231.655912	6628.238346	8.400179	-0.047146	4.396042
231.547161	6636.182191	8.405184	-0.047131	4.398588
231.924482	6644.196587	8.410189	-0.047206	4.401157
231.944692	6652.204154	8.415194	-0.047215	4.403720
231.989403	6660.210146	8.420198	-0.047229	4.406282
232.132243	6668.278820	8.425203	-0.047260	4.408863
232.433309	6676.283314	8.430208	-0.047321	4.411422
232.504287	6684.306957	8.435213	-0.047340	4.413985
232.803588	6692.366978	8.440218	-0.047401	4.416559
232.819979	6700.312811	8.445222	-0.047409	4.419094
233.032059	6708.412089	8.450227	-0.047453	4.421677
233.147153	6716.391208	8.455232	-0.047480	4.424220
233.533515	6724.420006	8.460237	-0.047557	4.426778
233.814220	6732.433559	8.465242	-0.047614	4.429330
233.447160	6740.472930	8.470246	-0.047551	4.431885
233.765898	6748.488429	8.475251	-0.047616	4.434435
234.158455	6756.513541	8.480256	-0.047694	4.436986
234.188430	6764.470727	8.485261	-0.047704	4.439513
234.378418	6772.549371	8.490266	-0.047745	4.442077
234.411251	6780.468457	8.495270	-0.047756	4.444589
234.914703	6788.554316	8.500275	-0.047855	4.447154
234.895105	6796.550304	8.505280	-0.047856	4.449687
234.917845	6804.575952	8.510285	-0.047866	4.452228
235.060886	6812.594816	8.515290	-0.047897	4.454765
235.132529	6820.623152	8.520294	-0.047916	4.457305
235.228664	6828.607387	8.525299	-0.047939	4.459828
235.392020	6836.652724	8.530304	-0.047974	4.462370
235.579727	6844.627252	8.535309	-0.048014	4.464888
235.747720	6852.717449	8.540314	-0.048051	4.467442
236.001387	6860.671729	8.545318	-0.048103	4.469951
236.119176	6868.719313	8.550323	-0.048130	4.472487
236.254771	6876.739595	8.555328	-0.048161	4.475014
236.515876	6884.739301	8.560333	-0.048214	4.477533
236.733006	6892.757988	8.565338	-0.048260	4.480057
236.610837	6900.710349	8.570343	-0.048242	4.482557
236.773455	6908.749647	8.575347	-0.048278	4.485084
236.882769	6916.786132	8.580352	-0.048303	4.487608
237.410788	6924.799183	8.585357	-0.048406	4.490125
237.321378	6932.845817	8.590362	-0.048395	4.492649
237.626290	6940.859345	8.595367	-0.048457	4.495163
237.800096	6948.905610	8.600371	-0.048494	4.497685
237.726824	6956.869972	8.605376	-0.048486	4.500179
237.984219	6964.851750	8.610381	-0.048539	4.502678
238.451436	6972.871183	8.615386	-0.048631	4.505188
238.474393	6980.917039	8.620391	-0.048640	4.507704
238.692997	6988.963781	8.625395	-0.048686	4.510219
238.889371	6996.999290	8.630400	-0.048728	4.512729
239.134227	7005.037974	8.635405	-0.048778	4.515239
239.461181	7013.026543	8.640410	-0.048844	4.517732
239.564569	7020.952234	8.645415	-0.048869	4.520203
239.721709	7028.992153	8.650419	-0.048903	4.522709
239.684065	7036.971812	8.655424	-0.048901	4.525194
239.812042	7045.027938	8.660429	-0.048930	4.527702
239.965686	7053.041235	8.665434	-0.048964	4.530195
240.170203	7061.070733	8.670439	-0.049007	4.532692
240.184550	7069.061740	8.675443	-0.049015	4.535175
240.313481	7077.114751	8.680448	-0.049044	4.537677
240.552993	7085.070998	8.685453	-0.049093	4.540147
240.847756	7093.177317	8.690458	-0.049154	4.542662
240.743857	7101.112212	8.695463	-0.049139	4.545122
240.932451	7109.184828	8.700467	-0.049179	4.547624
240.967637	7117.180091	8.705472	-0.049191	4.550101
241.239151	7125.214866	8.710477	-0.049247	4.552588
241.375173	7133.247735	8.715482	-0.049277	4.555074
241.431239	7141.258154	8.720487	-0.049293	4.557551
241.699135	7149.218466	8.725491	-0.049348	4.560011
241.901169	7157.261319	8.730496	-0.049390	4.562496
241.924152	7165.210228	8.735501	-0.049400	4.564950
241.939323	7173.332489	8.740506	-0.049408	4.567456
242.097769	7181.246034	8.745511	-0.049442	4.569896
242.515810	7189.370700	8.750515	-0.049525	4.572401
242.600382	7197.342922	8.755520	-0.049546	4.574856
242.620944	7205.384583	8.760525	-0.049555	4.577332
242.691864	7213.357395	8.765530	-0.049573	4.579785
242.843730	7221.392182	8.770535	-0.049607	4.582256
242.956240	7229.421311	8.775539	-0.049633	4.584724
243.177235	7237.443388	8.780544	-0.049679	4.587189
243.201874	7245.442820	8.785549	-0.049689	4.589645
243.348585	7253.513489	8.790554	-0.049721	4.592122
243.476815	7261.534646	8.795559	-0.049750	4.594582
243.804746	7269.610799	8.800563	-0.049816	4.597058
243.818872	7277.477794	8.805568	-0.049824	4.599468
243.944163	7285.530338	8.810573	-0.049852	4.601933
244.087247	7293.529078	8.815578	-0.049884	4.604381
244.259696	7301.573976	8.820583	-0.049921	4.606842
244.343326	7309.590608	8.825587	-0.049942	4.609293
244.528218	7317.598227	8.830592	-0.049982	4.611740
244.738665	7325.610175	8.835597	-0.050026	4.614186
245.187291	7333.716516	8.840602	-0.050115	4.616661
245.123157	7341.599996	8.845607	-0.050108	4.619065
245.281552	7349.678175	8.850611	-0.050142	4.621528
245.480595	7357.639833	8.855616	-0.050184	4.623955
245.656552	7365.692891	8.860621	-0.050222	4.626407
245.809301	7373.707188	8.865626	-0.050256	4.628847
245.614086	7381.721248	8.870631	-0.050225	4.631285
245.892903	7389.780187	8.875635	-0.050282	4.633735
246.192401	7397.791139	8.880640	-0.050343	4.636170
246.248033	7405.738132	8.885645	-0.050358	4.638584
246.482940	7413.797655	8.890650	-0.050407	4.641031
246.406550	7421.732203	8.895655	-0.050398	4.643438
246.601291	7429.777553	8.900659	-0.050439	4.645878
246.853030	7437.810878	8.905664	-0.050491	4.648313
246.858727	7445.780837	8.910669	-0.050497	4.650728
247.051426	7453.900919	8.915674	-0.050538	4.653186
247.152662	7461.872372	8.920679	-0.050562	4.655599
247.413219	7469.893969	8.925683	-0.050616	4.658025
247.386607	7477.880614	8.930688	-0.050616	4.660439
247.639772	7485.910688	8.935693	-0.050668	4.662865
247.650854	7493.928583	8.940698	-0.050675	4.665287
247.704551	7501.957040	8.945703	-0.050690	4.667710
247.956699	7509.940872	8.950707	-0.050742	4.670118
248.050271	7518.058705	8.955712	-0.050765	4.672566
248.058998	7526.098577	8.960717	-0.050772	4.674989
248.314680	7534.038100	8.965722	-0.050824	4.677380
248.322807	7542.002308	8.970727	-0.050831	4.679778
248.641340	7550.061510	8.975731	-0.050895	4.682202
248.640228	7558.008004	8.980736	-0.050900	4.684592
248.807261	7566.050942	8.985741	-0.050936	4.687010
248.971654	7574.054434	8.990746	-0.050972	4.689414
249.092318	7582.081597	8.995751	-0.051000	4.691824
249.314848	7590.084448	9.000755	-0.051046	4.694226
249.513378	7598.177742	9.005760	-0.051088	4.696653
249.480109	7606.097733	9.010765	-0.051087	4.699027
249.646304	7614.117926	9.015770	-0.051123	4.701430
249.984510	7622.147679	9.020775	-0.051191	4.703835
250.010747	7630.177329	9.025779	-0.051201	4.706238
250.091501	7638.207333	9.030784	-0.051222	4.708641
250.308698	7646.214324	9.035789	-0.051267	4.711035
250.555171	7654.292577	9.040794	-0.051318	4.713449
250.629738	7662.226299	9.045799	-0.051337	4.715819
250.675423	7670.261076	9.050803	-0.051351	4.718217
250.900259	7678.226136	9.055808	-0.051398	4.720594
250.932725	7686.257509	9.060813	-0.051409	4.722989
251.001925	7694.302730	9.065818	-0.051427	4.725388
251.071361	7702.302818	9.070823	-0.051445	4.727771
251.430953	7710.352639	9.075827	-0.051517	4.730168
251.509196	7718.411387	9.080832	-0.051537	4.732567
251.761465	7726.398261	9.085837	-0.051589	4.734942
251.928225	7734.444070	9.090842	-0.051625	4.737334
251.803639	7742.398649	9.095847	-0.051607	4.739699
252.005421	7750.423554	9.100851	-0.051649	4.742082
252.163749	7758.438458	9.105856	-0.051684	4.744461
252.151123	7766.433550	9.110861	-0.051687	4.746834
252.365471	7774.476147	9.115866	-0.051732	4.749219
252.377956	7782.504864	9.120871	-0.051739	4.751599
252.721254	7790.584518	9.125875	-0.051808	4.753992
252.741220	7798.571926	9.130880	-0.051817	4.756358
252.918588	7806.506066	9.135885	-0.051855	4.758706
253.209790	7814.566913	9.140890	-0.051914	4.761090
253.190753	7822.530012	9.145895	-0.051916	4.763445
253.299073	7830.573608	9.150899	-0.051941	4.765822
253.740059	7838.587314	9.155904	-0.052028	4.768188
253.546421	7846.584544	9.160909	-0.051997	4.770550
253.695405	7854.649279	9.165914	-0.052030	4.772929
253.924311	7862.627033	9.170919	-0.052078	4.775282
254.211185	7870.651942	9.175923	-0.052137	4.777647
254.175251	7878.674535	9.180928	-0.052135	4.780011
254.170271	7886.641079	9.185933	-0.052139	4.782357
254.592799	7894.673608	9.190938	-0.052223	4.784721
254.554833	7902.685847	9.195943	-0.052221	4.787078
254.797721	7910.702795	9.200947	-0.052271	4.789435
255.050798	7918.743060	9.205952	-0.052323	4.791797
255.171278	7926.755720	9.210957	-0.052351	4.794151
255.238407	7934.831139	9.215962	-0.052369	4.796522
255.415902	7942.736681	9.220967	-0.052407	4.798842
255.673447	7950.825087	9.225971	-0.052460	4.801214
255.544295	7958.796690	9.230976	-0.052441	4.803552
255.615203	7966.780550	9.235981	-0.052459	4.805891
256.130240	7974.849897	9.240986	-0.052560	4.808253
256.007454	7982.851464	9.245991	-0.052542	4.810596
256.160933	7990.245633	9.250995	-0.052576	4.812760
256.369699	7994.755652	9.256000	-0.052617	4.814078

256.439912	7997.189388	9.261005	-0.052632	4.814789
256.353745	7998.463673	9.266010	-0.052617	4.815163
256.541879	7998.912961	9.271015	-0.052652	4.815293
256.729691	7999.918505	9.276019	-0.052687	4.815586
256.631039	7999.894472	9.281024	-0.052669	4.815580
256.697023	7999.921156	9.286029	-0.052681	4.815587
256.903422	7999.890332	9.291034	-0.052719	4.815577
256.803022	7999.871608	9.296039	-0.052700	4.815572
256.931492	7999.912120	9.301043	-0.052724	4.815583
256.848573	7999.884071	9.306048	-0.052709	4.815576
257.043378	7999.864803	9.311053	-0.052745	4.815569
257.188222	7999.905581	9.316058	-0.052772	4.815580
257.002012	7999.859839	9.321063	-0.052737	4.815568
257.231951	7999.899864	9.326067	-0.052780	4.815578
257.243617	7999.884028	9.331072	-0.052782	4.815574
256.992215	7999.893813	9.336077	-0.052735	4.815578
257.378807	7999.922503	9.341082	-0.052807	4.815584
257.365736	7999.885979	9.346087	-0.052804	4.815574
257.328066	7999.901372	9.351091	-0.052797	4.815578
257.415411	7999.902780	9.356096	-0.052813	4.815578
257.411689	7999.904844	9.361101	-0.052812	4.815579
257.463736	7999.893934	9.366106	-0.052822	4.815576
257.592012	7999.915226	9.371111	-0.052845	4.815581
257.657150	7999.929086	9.376115	-0.052858	4.815585
257.741142	7999.915492	9.381120	-0.052873	4.815581
257.586433	7999.911900	9.386125	-0.052844	4.815580
257.706113	7999.949067	9.391130	-0.052866	4.815591
257.612845	7999.905901	9.396135	-0.052849	4.815578
257.644874	7999.940577	9.401139	-0.052855	4.815588
257.794781	7999.912039	9.406144	-0.052882	4.815579
257.686313	7999.893183	9.411149	-0.052862	4.815574
257.859150	7999.892777	9.416154	-0.052894	4.815573
257.699174	7999.881626	9.421159	-0.052864	4.815571
257.854052	7999.922568	9.426163	-0.052893	4.815582
258.031391	7999.915830	9.431168	-0.052926	4.815579
257.876157	7999.904755	9.436173	-0.052897	4.815577
257.905106	7999.943652	9.441178	-0.052902	4.815588
257.914497	7999.889341	9.446183	-0.052904	4.815572
258.061721	7999.916280	9.451187	-0.052931	4.815579
258.092215	7999.917832	9.456192	-0.052937	4.815580
257.949792	7999.892018	9.461197	-0.052910	4.815573
257.864287	7999.929055	9.466202	-0.052894	4.815584
257.998150	7999.895985	9.471207	-0.052919	4.815574
258.188771	7999.919358	9.476211	-0.052954	4.815580
258.146782	7999.903717	9.481216	-0.052946	4.815575
258.018704	7999.903761	9.486221	-0.052922	4.815576
258.169401	7999.933959	9.491226	-0.052950	4.815584
258.015103	7999.917561	9.496231	-0.052921	4.815580
258.259330	7999.932196	9.501235	-0.052967	4.815583
258.190635	7999.911850	9.506240	-0.052954	4.815577
258.121372	7999.889360	9.511245	-0.052941	4.815571
258.220555	7999.936872	9.516250	-0.052959	4.815585
258.259099	7999.899050	9.521255	-0.052966	4.815573
258.176128	7999.945738	9.526259	-0.052950	4.815587
258.173839	7999.920065	9.531264	-0.052950	4.815580
258.113786	7999.923350	9.536269	-0.052939	4.815581
258.473851	7999.925987	9.541274	-0.053006	4.815580
258.216375	7999.912183	9.546279	-0.052957	4.815577
258.207514	7999.915231	9.551283	-0.052956	4.815578
258.268289	7999.903396	9.556288	-0.052967	4.815575
258.319722	7999.910627	9.561293	-0.052976	4.815577
258.443810	7999.930784	9.566298	-0.052999	4.815582
258.466663	7999.907655	9.571303	-0.053003	4.815575
258.316990	7999.916956	9.576307	-0.052975	4.815578
258.523486	7999.910692	9.581312	-0.053014	4.815576
258.323220	7999.906359	9.586317	-0.052976	4.815575
258.419087	7999.920719	9.591322	-0.052994	4.815579
258.246844	7999.874133	9.596327	-0.052962	4.815566
258.358646	7999.916512	9.601331	-0.052983	4.815578
258.352218	7999.920668	9.606336	-0.052981	4.815579
258.286873	7999.901444	9.611341	-0.052969	4.815574
258.394398	7999.915993	9.616346	-0.052989	4.815578
258.311789	7999.896489	9.621351	-0.052973	4.815572
258.344600	7999.917298	9.626355	-0.052979	4.815578
258.435553	7999.898479	9.631360	-0.052996	4.815572
258.169657	7999.887741	9.636365	-0.052947	4.815571
258.427184	7999.942097	9.641370	-0.052994	4.815585
258.300853	7999.891987	9.646375	-0.052971	4.815571
258.418400	7999.939798	9.651379	-0.052993	4.815585
258.528110	7999.913810	9.656384	-0.053013	4.815577
258.393654	7999.894530	9.661389	-0.052988	4.815572
258.526339	7999.906285	9.666394	-0.053012	4.815574
258.540995	7999.896903	9.671399	-0.053015	4.815572
258.675169	7999.924699	9.676403	-0.053040	4.815579
258.733354	7999.919227	9.681408	-0.053050	4.815577
258.667414	7999.897858	9.686413	-0.053038	4.815571
258.685981	7999.923774	9.691418	-0.053041	4.815579
258.626856	7999.901448	9.696423	-0.053030	4.815572
258.731608	7999.929833	9.701427	-0.053050	4.815580
258.730341	7999.934073	9.706432	-0.053049	4.815582
258.701536	7999.886614	9.711437	-0.053044	4.815568
258.873730	7999.935314	9.716442	-0.053076	4.815581
258.814560	7999.895904	9.721447	-0.053065	4.815570
258.581376	7999.925202	9.726451	-0.053021	4.815580
258.718851	7999.915681	9.731456	-0.053046	4.815576
258.670096	7999.909539	9.736461	-0.053037	4.815575
258.641456	7999.904792	9.741466	-0.053032	4.815573
258.701643	7999.881202	9.746471	-0.053043	4.815566
258.722276	7999.908220	9.751475	-0.053047	4.815574
258.821837	7999.922640	9.756480	-0.053065	4.815578
258.677127	7999.913871	9.761485	-0.053038	4.815576
258.844496	7999.903768	9.766490	-0.053069	4.815572
258.593895	7999.871924	9.771495	-0.053022	4.815564
258.457508	7999.917743	9.776499	-0.052997	4.815578
258.668910	7999.924372	9.781504	-0.053036	4.815579
258.461968	7999.918862	9.786509	-0.052997	4.815578
258.467647	7999.974465	9.791514	-0.052998	4.815595
258.540920	7999.901973	9.796519	-0.053012	4.815573
258.678459	7999.919145	9.801523	-0.053037	4.815577
258.761516	7999.918349	9.806528	-0.053053	4.815577
258.665636	7999.902900	9.811533	-0.053035	4.815573
258.890889	7999.926837	9.816538	-0.053076	4.815579
258.911979	7999.905814	9.821543	-0.053080	4.815572
258.635739	7999.938684	9.826547	-0.053029	4.815583
258.735254	7999.928546	9.831552	-0.053047	4.815580
258.662769	7999.898529	9.836557	-0.053033	4.815572
258.696692	7999.931101	9.841562	-0.053040	4.815581
258.775231	7999.896064	9.846567	-0.053054	4.815570
258.794405	7999.905974	9.851571	-0.053058	4.815573
258.867716	7999.919968	9.856576	-0.053071	4.815577
258.778214	7999.908893	9.861581	-0.053054	4.815574
258.801385	7999.944494	9.866586	-0.053059	4.815584
258.658931	7999.882375	9.871591	-0.053032	4.815567
258.602198	7999.910271	9.876595	-0.053021	4.815575
258.658982	7999.893032	9.881600	-0.053032	4.815570
258.947591	7999.892373	9.886605	-0.053085	4.815568
258.840818	7999.935471	9.891610	-0.053065	4.815582
258.850740	7999.923877	9.896615	-0.053067	4.815578
258.918621	7999.924970	9.901619	-0.053079	4.815578
258.817439	7999.920111	9.906624	-0.053061	4.815577
258.720785	7999.893972	9.911629	-0.053042	4.815570
258.793401	7999.927173	9.916634	-0.053056	4.815579
258.956649	7999.904191	9.921639	-0.053086	4.815572
258.864846	7999.921907	9.926643	-0.053069	4.815577
258.930725	7999.918696	9.931648	-0.053081	4.815576
259.047594	7999.905637	9.936653	-0.053103	4.815572
258.999337	7999.929399	9.941658	-0.053094	4.815579
258.912050	7999.899141	9.946663	-0.053077	4.815571
258.990010	7999.932429	9.951667	-0.053092	4.815580
258.860872	7999.928184	9.956672	-0.053067	4.815579
258.702090	7999.875410	9.961677	-0.053038	4.815565
258.992383	7999.924962	9.966682	-0.053092	4.815578
258.980566	7999.911946	9.971687	-0.053089	4.815574
258.952005	7999.914674	9.976691	-0.053084	4.815575
258.863001	7999.903607	9.981696	-0.053067	4.815572
258.813816	7999.908136	9.986701	-0.053058	4.815574
259.016206	7999.937040	9.991706	-0.053095	4.815581
258.871556	7999.918662	9.996711	-0.053068	4.815577
258.982198	7999.910840	10.001715	-0.053089	4.815574
258.872210	7999.921855	10.006720	-0.053068	4.815577
258.854510	7999.898066	10.011725	-0.053065	4.815571
259.018062	7999.945558	10.016730	-0.053095	4.815584
258.960849	7999.923263	10.021735	-0.053084	4.815577
258.947823	7999.948666	10.026739	-0.053082	4.815585
258.928652	7999.948344	10.031744	-0.053078	4.815585
258.906027	7999.924475	10.036749	-0.053074	4.815578
259.100383	7999.928692	10.041754	-0.053110	4.815578
258.989725	7999.899121	10.046759	-0.053089	4.815570
258.830397	7999.912537	10.051763	-0.053059	4.815575
259.000682	7999.922768	10.056768	-0.053091	4.815577
258.758564	7999.899603	10.061773	-0.053046	4.815572
258.836797	7999.929692	10.066778	-0.053060	4.815580
259.067248	7999.920615	10.071783	-0.053103	4.815576
259.031045	7999.928557	10.076787	-0.053096	4.815579
259.180649	7999.904285	10.081792	-0.053124	4.815571
259.137924	7999.897174	10.086797	-0.053116	4.815569
259.146211	7999.956023	10.091802	-0.053117	4.815586
258.976082	7999.911605	10.096807	-0.053085	4.815574
259.072484	7999.915297	10.101811	-0.053103	4.815575
259.368637	7999.899814	10.106816	-0.053158	4.815569
259.063340	7999.888434	10.111821	-0.053101	4.815567
259.156030	7999.934774	10.116826	-0.053118	4.815580
259.279594	7999.895131	10.121831	-0.053141	4.815568
259.128425	7999.912949	10.126835	-0.053113	4.815574
259.209872	7999.922804	10.131840	-0.053128	4.815576
259.185907	7999.907456	10.136845	-0.053123	4.815572
259.306549	7999.909406	10.141850	-0.053146	4.815572
259.155989	7999.880255	10.146855	-0.053118	4.815564
259.041683	7999.927501	10.151859	-0.053096	4.815578
259.264930	7999.918307	10.156864	-0.053138	4.815575
259.150208	7999.897212	10.161869	-0.053116	4.815569
259.101071	7999.917757	10.166874	-0.053107	4.815575
259.066860	7999.918258	10.171879	-0.053100	4.815576
259.088002	7999.912185	10.176883	-0.053104	4.815574
259.222857	7999.939992	10.181888	-0.053129	4.815581
259.237214	7999.933808	10.186893	-0.053132	4.815579
259.148768	7999.957985	10.191898	-0.053115	4.815587
259.168922	7999.919864	10.196903	-0.053119	4.815576
259.014684	7999.901330	10.201907	-0.053090	4.815571
259.151620	7999.903545	10.206912	-0.053115	4.815571
259.078618	7999.886332	10.211917	-0.053102	4.815566
259.142648	7999.932206	10.216922	-0.053113	4.815579
259.135041	7999.906447	10.221927	-0.053112	4.815572
259.115316	7999.922131	10.226931	-0.053108	4.815577
259.044287	7999.932711	10.231936	-0.053095	4.815580
258.919958	7999.909325	10.236941	-0.053071	4.815574
258.975639	7999.915558	10.241946	-0.053082	4.815575
259.074219	7999.903269	10.246951	-0.053100	4.815571
259.139207	7999.914992	10.251955	-0.053112	4.815574
259.262431	7999.927661	10.256960	-0.053135	4.815577
259.176069	7999.917705	10.261965	-0.053119	4.815575
259.064056	7999.953244	10.266970	-0.053098	4.815586
259.108921	7999.935811	10.271975	-0.053106	4.815581
259.177910	7999.927312	10.276979	-0.053119	4.815578
259.039779	7999.925056	10.281984	-0.053093	4.815578
259.013157	7999.905394	10.286989	-0.053088	4.815572
259.223785	7999.916281	10.291994	-0.053127	4.815574
259.169701	7999.913255	10.296999	-0.053117	4.815574
259.126283	7999.916810	10.302003	-0.053108	4.815575
259.272437	7999.912769	10.307008	-0.053135	4.815573
258.937002	7999.904102	10.312013	-0.053073	4.815572
259.228717	7999.929120	10.317018	-0.053127	4.815578
259.227651	7999.913076	10.322023	-0.053127	4.815573
259.170342	7999.933488	10.327027	-0.053116	4.815580
259.276770	7999.939479	10.332032	-0.053136	4.815581
259.161699	7999.913040	10.337037	-0.053114	4.815574
259.204503	7999.923334	10.342042	-0.053122	4.815577
259.197985	7999.900795	10.347047	-0.053121	4.815570
259.041037	7999.930265	10.352051	-0.053091	4.815579
259.252510	7999.909134	10.357056	-0.053130	4.815572
259.017186	7999.898892	10.362061	-0.053087	4.815570
258.999141	7999.928484	10.367066	-0.053083	4.815579
259.329904	7999.905022	10.372071	-0.053145	4.815571
259.337805	7999.909410	10.377075	-0.053146	4.815572
259.384089	7999.928303	10.382080	-0.053154	4.815577
259.335727	7999.914694	10.387085	-0.053145	4.815573
259.447802	7999.931453	10.392090	-0.053166	4.815578
259.298362	7999.919403	10.397095	-0.053138	4.815575
259.294082	7999.931068	10.402099	-0.053137	4.815578
259.317372	7999.932504	10.407104	-0.053141	4.815579
259.325955	7999.907007	10.412109	-0.053143	4.815571
259.347397	7999.935106	10.417114	-0.053147	4.815579
259.183073	7999.916408	10.422119	-0.053116	4.815575
259.176820	7999.907754	10.427123	-0.053115	4.815572
259.228635	7999.903247	10.432128	-0.053124	4.815571
259.245088	7999.912045	10.437133	-0.053127	4.815573
259.237410	7999.914045	10.442138	-0.053126	4.815574
259.425715	7999.910689	10.447143	-0.053161	4.815572
259.427265	7999.910704	10.452147	-0.053161	4.815572
259.427356	7999.908559	10.457152	-0.053161	4.815571
259.451406	7999.872636	10.462157	-0.053165	4.815561
259.570678	7999.943967	10.467162	-0.053187	4.815581
259.240023	7999.909752	10.472167	-0.053125	4.815572
259.382513	7999.919532	10.477171	-0.053152	4.815575
259.533318	7999.926244	10.482176	-0.053180	4.815576
259.212603	7999.888987	10.487181	-0.053120	4.815567
259.393583	7999.919680	10.492186	-0.053153	4.815575
259.547061	7999.918961	10.497191	-0.053182	4.815574
259.263721	7999.906870	10.502195	-0.053129	4.815572
259.433975	7999.925643	10.507200	-0.053161	4.815576
259.391538	7999.911062	10.512205	-0.053153	4.815572
259.302421	7999.924550	10.517210	-0.053136	4.815577
259.296401	7999.909494	10.522215	-0.053135	4.815572
259.471248	7999.911258	10.527219	-0.053167	4.815572
259.445034	7999.954598	10.532224	-0.053162	4.815585
259.152278	7999.900712	10.537229	-0.053107	4.815570
259.254084	7999.939727	10.542234	-0.053126	4.815581
259.415158	7999.894287	10.547239	-0.053156	4.815567
259.324743	7999.904551	10.552243	-0.053139	4.815571
259.391150	7999.922704	10.557248	-0.053151	4.815576
259.450371	7999.912979	10.562253	-0.053162	4.815572
259.511819	7999.918238	10.567258	-0.053174	4.815574
259.522096	7999.894904	10.572263	-0.053175	4.815567
259.611407	7999.903819	10.577267	-0.053192	4.815569
259.631441	7999.937234	10.582272	-0.053196	4.815579
259.338446	7999.929257	10.587277	-0.053141	4.815578
259.657869	7999.949388	10.592282	-0.053200	4.815582
259.468838	7999.916407	10.597287	-0.053165	4.815573
259.432972	7999.925423	10.602291	-0.053158	4.815576
259.471348	7999.913223	10.607296	-0.053165	4.815572
259.504892	7999.904148	10.612301	-0.053171	4.815570
259.508801	7999.926623	10.617306	-0.053172	4.815576
259.473770	7999.929246	10.622311	-0.053165	4.815577
259.299842	7999.907189	10.627315	-0.053133	4.815572
259.442751	7999.939398	10.632320	-0.053159	4.815580
259.442685	7999.899880	10.637325	-0.053159	4.815569
259.409578	7999.936702	10.642330	-0.053153	4.815580
259.681214	7999.912278	10.647335	-0.053203	4.815571
259.508960	7999.921212	10.652339	-0.053171	4.815575
259.551288	7999.925093	10.657344	-0.053179	4.815576
259.508648	7999.908373	10.662349	-0.053171	4.815571
259.612153	7999.933535	10.667354	-0.053190	4.815578
259.682710	7999.903707	10.672359	-0.053203	4.815569
259.517600	7999.892470	10.677363	-0.053172	4.815566
259.570415	7999.931757	10.682368	-0.053182	4.815577
259.309480	7999.895472	10.687373	-0.053133	4.815568
259.693752	7999.928402	10.692378	-0.053204	4.815576
259.561912	7999.895283	10.697383	-0.053180	4.815567
259.654220	7999.901044	10.702387	-0.053197	4.815568
259.812009	7999.933496	10.707392	-0.053226	4.815577
259.622210	7999.932534	10.712397	-0.053191	4.815577
259.614749	7999.939876	10.717402	-0.053189	4.815580
259.488893	7999.948497	10.722407	-0.053166	4.815583
259.473955	7999.936498	10.727411	-0.053163	4.815579
259.737755	7999.920489	10.732416	-0.053212	4.815573
259.716926	7999.907327	10.737421	-0.053208	4.815570
259.566086	7999.913406	10.742426	-0.053179	4.815572
259.556963	7999.908976	10.747431	-0.053178	4.815571
259.553454	7999.917450	10.752435	-0.053177	4.815573
259.594573	7999.922379	10.757440	-0.053184	4.815575
259.463864	7999.910633	10.762445	-0.053160	4.815572
259.454015	7999.933953	10.767450	-0.053158	4.815579
259.380751	7999.916735	10.772455	-0.053144	4.815574
259.452947	7999.927507	10.777459	-0.053157	4.815577
259.760605	7999.933567	10.782464	-0.053215	4.815577
259.494356	7999.918550	10.787469	-0.053165	4.815574
259.501824	7999.934676	10.792474	-0.053166	4.815579
259.612391	7999.955682	10.797479	-0.053187	4.815584
259.637848	7999.944340	10.802483	-0.053191	4.815581
259.528223	7999.956428	10.807488	-0.053171	4.815585
259.581553	7999.930591	10.812493	-0.053181	4.815577
259.540695	7999.951271	10.817498	-0.053173	4.815583
259.802710	7999.928827	10.822503	-0.053221	4.815576
259.669934	7999.915980	10.827507	-0.053197	4.815572
259.804400	7999.942713	10.832512	-0.053222	4.815580
259.556759	7999.903441	10.837517	-0.053175	4.815569
259.557067	7999.914112	10.842522	-0.053175	4.815572
259.585384	7999.901749	10.847527	-0.053180	4.815569
259.715700	7999.924144	10.852531	-0.053205	4.815575
259.631777	7999.928108	10.857536	-0.053189	4.815576
259.625667	7999.908778	10.862541	-0.053188	4.815571
259.859150	7999.939257	10.867546	-0.053231	4.815578
259.803996	7999.942621	10.872551	-0.053221	4.815580
259.663084	7999.941387	10.877555	-0.053194	4.815580
259.764995	7999.943033	10.882560	-0.053213	4.815580
259.836458	7999.908949	10.887565	-0.053226	4.815570
259.756795	7999.975978	10.892570	-0.053211	4.815590
259.877649	7999.946968	10.897575	-0.053234	4.815581
259.810063	7999.917029	10.902579	-0.053221	4.815572
259.677478	7999.939421	10.907584	-0.053196	4.815579
259.772982	7999.900389	10.912589	-0.053214	4.815567
259.811448	7999.937307	10.917594	-0.053221	4.815578
259.851878	7999.906989	10.922599	-0.053228	4.815569
259.672536	7999.912604	10.927603	-0.053195	4.815572
259.812986	7999.921283	10.932608	-0.053221	4.815573
259.730426	7999.887898	10.937613	-0.053205	4.815564
259.641403	7999.927014	10.942618	-0.053189	4.815576
259.836897	7999.913098	10.947623	-0.053225	4.815571
259.815435	7999.923416	10.952627	-0.053221	4.815574
259.835605	7999.940817	10.957632	-0.053224	4.815579
259.672602	7999.918936	10.962637	-0.053194	4.815573
259.904853	7999.941921	10.967642	-0.053237	4.815579
259.852341	7999.946396	10.972647	-0.053227	4.815581
259.670555	7999.931684	10.977651	-0.053193	4.815577
259.727703	7999.930467	10.982656	-0.053204	4.815577
259.960235	7999.918221	10.987661	-0.053247	4.815572
259.595726	7999.930435	10.992666	-0.053179	4.815577
259.614484	7999.901900	10.997671	-0.053182	4.815569
259.468943	7999.898456	11.002675	-0.053155	4.815568
259.742492	7999.911434	11.007680	-0.053206	4.815571
259.714104	7999.909894	11.012685	-0.053200	4.815571
259.813253	7999.937121	11.017690	-0.053219	4.815578
260.113391	7999.913162	11.022695	-0.053274	4.815570
259.707405	7999.919363	11.027699	-0.053199	4.815573
259.947759	7999.940344	11.032704	-0.053243	4.815578
260.068381	7999.925211	11.037709	-0.053266	4.815573
259.829247	7999.925583	11.042714	-0.053221	4.815575
259.929747	7999.911190	11.047719	-0.053240	4.815570
259.860805	7999.901516	11.052723	-0.053227	4.815567
259.910854	7999.945029	11.057728	-0.053236	4.815580
259.822553	7999.920092	11.062733	-0.053219	4.815573
259.623537	7999.932862	11.067738	-0.053182	4.815578
259.962484	7999.913804	11.072743	-0.053245	4.815571
259.940795	7999.914508	11.077747	-0.053241	4.815571
259.906572	7999.933161	11.082752	-0.053234	4.815577
259.684218	7999.914586	11.087757	-0.053193	4.815572
259.910744	7999.926801	11.092762	-0.053235	4.815575
260.035872	7999.926689	11.097767	-0.053258	4.815574
259.945753	7999.897452	11.102771	-0.053241	4.815566
259.959942	7999.946788	11.107776	-0.053244	4.815580
259.880091	7999.910243	11.112781	-0.053229	4.815570
259.892211	7999.914700	11.117786	-0.053231	4.815571
260.054602	7999.934414	11.122791	-0.053261	4.815576
259.868022	7999.919624	11.127795	-0.053226	4.815573
260.014165	7999.948684	11.132800	-0.053253	4.815581
260.004499	7999.942109	11.137805	-0.053251	4.815579
259.955662	7999.944507	11.142810	-0.053242	4.815580
259.947831	7999.908066	11.147815	-0.053241	4.815569
259.854586	7999.918284	11.152819	-0.053223	4.815572
259.979266	7999.911759	11.157824	-0.053246	4.815570
259.749117	7999.912277	11.162829	-0.053203	4.815571
259.834056	7999.920054	11.167834	-0.053219	4.815573
260.131848	7999.960121	11.172839	-0.053274	4.815583
259.992785	7999.917275	11.177843	-0.053248	4.815572
259.905461	7999.950012	11.182848	-0.053232	4.815582
259.840771	7999.930798	11.187853	-0.053220	4.815576
259.942821	7999.930311	11.192858	-0.053238	4.815576
259.851855	7999.925618	11.197863	-0.053221	4.815575
259.838818	7999.931801	11.202867	-0.053219	4.815577
260.036430	7999.978782	11.207872	-0.053256	4.815589
259.823930	7999.936876	11.212877	-0.053216	4.815578
260.035609	7999.924292	11.217882	-0.053255	4.815573
260.055209	7999.917125	11.222887	-0.053259	4.815571
259.871305	7999.916260	11.227891	-0.053224	4.815572
259.874394	7999.940857	11.232896	-0.053225	4.815579
260.085160	7999.897293	11.237901	-0.053264	4.815565
260.090738	7999.921931	11.242906	-0.053265	4.815572
259.979747	7999.927590	11.247911	-0.053244	4.815575
259.893613	7999.934720	11.252915	-0.053228	4.815577
260.018439	7999.946349	11.257920	-0.053251	4.815580
259.910864	7999.918963	11.262925	-0.053231	4.815572
259.851388	7999.929731	11.267930	-0.053220	4.815576
259.940447	7999.920491	11.272935	-0.053236	4.815573
259.884032	7999.909953	11.277939	-0.053225	4.815570
259.914249	7999.930721	11.282944	-0.053231	4.815576
260.058812	7999.931993	11.287949	-0.053258	4.815576
260.056811	7999.921272	11.292954	-0.053257	4.815572
260.104499	7999.935918	11.297959	-0.053266	4.815577
259.975473	7999.907115	11.302963	-0.053242	4.815569
259.991361	7999.927650	11.307968	-0.053245	4.815575
259.972882	7999.916661	11.312973	-0.053241	4.815572
260.104235	7999.949751	11.317978	-0.053265	4.815581
260.164649	7999.920826	11.322983	-0.053277	4.815572
259.912196	7999.916710	11.327987	-0.053229	4.815572
259.942121	7999.923592	11.332992	-0.053235	4.815574
260.011196	7999.920434	11.337997	-0.053248	4.815572
259.987239	7999.925372	11.343002	-0.053243	4.815574
260.151090	7999.917349	11.348007	-0.053273	4.815571
259.955412	7999.904546	11.353011	-0.053237	4.815568
259.967954	7999.922891	11.358016	-0.053239	4.815573
259.813821	7999.896884	11.363021	-0.053210	4.815567
260.026896	7999.949454	11.368026	-0.053250	4.815581
260.250364	7999.922113	11.373031	-0.053291	4.815572
260.180188	7999.928435	11.378035	-0.053278	4.815574
260.141122	7999.930992	11.383040	-0.053271	4.815575
260.141232	7999.923509	11.388045	-0.053271	4.815573
260.112653	7999.931575	11.393050	-0.053265	4.815575
260.096869	7999.944121	11.398055	-0.053262	4.815579
259.932597	7999.917949	11.403059	-0.053231	4.815572
260.086812	7999.931123	11.408064	-0.053260	4.815575
260.013222	7999.917103	11.413069	-0.053246	4.815572
259.987614	7999.922014	11.418074	-0.053241	4.815573
259.861148	7999.895389	11.423079	-0.053218	4.815566
260.017908	7999.907537	11.428083	-0.053247	4.815569
259.954098	7999.936385	11.433088	-0.053235	4.815577
260.059040	7999.917794	11.438093	-0.053254	4.815572
260.189681	7999.951940	11.443098	-0.053278	4.815581
260.370220	7999.959137	11.448103	-0.053312	4.815582
260.164561	7999.923749	11.453107	-0.053273	4.815573
260.190131	7999.962593	11.458112	-0.053278	4.815584
260.146630	7999.929842	11.463117	-0.053270	4.815575
260.089994	7999.937452	11.468122	-0.053259	4.815577
260.007932	7999.919023	11.473127	-0.053244	4.815572
260.171570	7999.919538	11.478131	-0.053274	4.815572
260.213700	7999.950109	11.483136	-0.053282	4.815580
260.187721	7999.926186	11.488141	-0.053277	4.815573
260.301686	7999.926961	11.493146	-0.053298	4.815573
260.192701	7999.920906	11.498151	-0.053278	4.815572
260.210329	7999.900895	11.503155	-0.053281	4.815566
260.258424	7999.933699	11.508160	-0.053290	4.815575
259.902362	7999.920424	11.513165	-0.053223	4.815573
259.906398	7999.929021	11.518170	-0.053224	4.815576
259.889753	7999.925536	11.523175	-0.053220	4.815575
260.021105	7999.906307	11.528179	-0.053245	4.815568
260.066131	7999.940128	11.533184	-0.053253	4.815578
260.155471	7999.910605	11.538189	-0.053270	4.815569
260.249624	7999.943091	11.543194	-0.053287	4.815578
260.356583	7999.932006	11.548199	-0.053307	4.815574
260.073528	7999.898563	11.553203	-0.053254	4.815566
260.253284	7999.927102	11.558208	-0.053287	4.815573
259.979027	7999.909818	11.563213	-0.053236	4.815570
260.101136	7999.919267	11.568218	-0.053259	4.815572
260.075708	7999.940198	11.573223	-0.053254	4.815578
260.226154	7999.907398	11.578227	-0.053282	4.815568
260.027688	7999.912702	11.583232	-0.053245	4.815570
260.145481	7999.890049	11.588237	-0.053266	4.815563
260.192989	7999.903623	11.593242	-0.053275	4.815567
260.245724	7999.913012	11.598247	-0.053285	4.815569
260.162835	7999.898840	11.603251	-0.053269	4.815566
260.251531	7999.918424	11.608256	-0.053286	4.815571
260.136843	7999.910142	11.613261	-0.053264	4.815569
260.173329	7999.928876	11.618266	-0.053271	4.815574
260.390873	7999.947351	11.623271	-0.053311	4.815579
260.179320	7999.926816	11.628275	-0.053272	4.815574
260.317270	7999.946133	11.633280	-0.053297	4.815579
260.121558	7999.913043	11.638285	-0.053261	4.815570
260.256443	7999.917361	11.643290	-0.053286	4.815571
260.259038	7999.918460	11.648295	-0.053286	4.815571
260.122764	7999.902353	11.653299	-0.053261	4.815567
260.234599	7999.920177	11.658304	-0.053281	4.815572
260.069130	7999.914272	11.663309	-0.053250	4.815571
260.213708	7999.948645	11.668314	-0.053277	4.815580
260.012825	7999.933622	11.673319	-0.053240	4.815577
260.118381	7999.926786	11.678323	-0.053259	4.815574
260.192688	7999.940796	11.683328	-0.053273	4.815578
260.015823	7999.904809	11.688333	-0.053240	4.815568
260.029312	7999.922102	11.693338	-0.053242	4.815573
260.223791	7999.906034	11.698343	-0.053278	4.815567
260.166713	7999.897621	11.703347	-0.053268	4.815565
260.197675	7999.937621	11.708352	-0.053273	4.815577
260.082205	7999.913309	11.713357	-0.053252	4.815570
260.087988	7999.924070	11.718362	-0.053253	4.815573
260.235818	7999.912583	11.723367	-0.053280	4.815569
260.077209	7999.915331	11.728371	-0.053250	4.815571
260.031875	7999.919922	11.733376	-0.053242	4.815572
259.993621	7999.900070	11.738381	-0.053235	4.815567
260.028816	7999.920919	11.743386	-0.053241	4.815573
260.287111	7999.913363	11.748391	-0.053289	4.815569
260.080004	7999.917459	11.753395	-0.053250	4.815572
260.172270	7999.912542	11.758400	-0.053267	4.815570
260.249047	7999.916983	11.763405	-0.053281	4.815571
260.207048	7999.926967	11.768410	-0.053274	4.815574
260.284798	7999.945304	11.773415	-0.053288	4.815579
260.248419	7999.906263	11.778419	-0.053281	4.815567
260.415114	7999.931386	11.783424	-0.053312	4.815574
260.315276	7999.909464	11.788429	-0.053293	4.815568
260.102293	7999.923074	11.793434	-0.053253	4.815573
260.317921	7999.927638	11.798439	-0.053293	4.815573
260.417837	7999.922845	11.803443	-0.053312	4.815572
260.195730	7999.923493	11.808448	-0.053270	4.815573
260.310313	7999.912533	11.813453	-0.053292	4.815569
260.211986	7999.952566	11.818458	-0.053273	4.815581
260.207995	7999.971709	11.823463	-0.053272	4.815587
260.344691	7999.922670	11.828467	-0.053298	4.815572
260.415689	7999.923814	11.833472	-0.053311	4.815572
260.307408	7999.926313	11.838477	-0.053291	4.815573
260.278469	7999.924764	11.843482	-0.053285	4.815573
260.410675	7999.938648	11.848487	-0.053310	4.815576
260.176821	7999.934835	11.853491	-0.053266	4.815576
260.105312	7999.962490	11.858496	-0.053252	4.815585
260.246436	7999.920997	11.863501	-0.053279	4.815572
260.200582	7999.924511	11.868506	-0.053270	4.815573
260.172661	7999.968892	11.873511	-0.053265	4.815586
260.030791	7999.927068	11.878515	-0.053238	4.815575
260.273259	7999.920322	11.883520	-0.053283	4.815572
260.253284	7999.917851	11.888525	-0.053279	4.815571
260.106066	7999.929327	11.893530	-0.053252	4.815575
260.278147	7999.912895	11.898535	-0.053284	4.815569
260.259130	7999.906169	11.903539	-0.053280	4.815567
260.301181	7999.929265	11.908544	-0.053288	4.815574
260.470223	7999.890361	11.913549	-0.053319	4.815562
260.415985	7999.908688	11.918554	-0.053309	4.815567
260.431308	7999.918536	11.923559	-0.053311	4.815570
260.351731	7999.923637	11.928563	-0.053297	4.815572
260.533490	7999.941531	11.933568	-0.053330	4.815577
260.469732	7999.910586	11.938573	-0.053318	4.815568
260.418380	7999.927892	11.943578	-0.053309	4.815573
260.463309	7999.944629	11.948583	-0.053317	4.815578
260.433970	7999.922786	11.953587	-0.053311	4.815572
260.192182	7999.955146	11.958592	-0.053266	4.815582
260.383356	7999.917670	11.963597	-0.053302	4.815570
260.440100	7999.934598	11.968602	-0.053312	4.815575
260.406779	7999.935113	11.973607	-0.053306	4.815575
260.413992	7999.911730	11.978611	-0.053307	4.815568
260.596140	7999.923223	11.983616	-0.053341	4.815571
260.526634	7999.917811	11.988621	-0.053328	4.815570
260.327157	7999.912421	11.993626	-0.053290	4.815569
260.441800	7999.921749	11.998631	-0.053312	4.815571
260.396989	7999.903925	12.003635	-0.053303	4.815566
260.447274	7999.939968	12.008640	-0.053312	4.815577
260.406999	7999.913676	12.013645	-0.053305	4.815569
260.357762	7999.925678	12.018650	-0.053295	4.815573
260.191028	7999.921888	12.023655	-0.053264	4.815572
260.124280	7999.899437	12.028659	-0.053252	4.815566
260.252907	7999.910060	12.033664	-0.053276	4.815569
260.204714	7999.893249	12.038669	-0.053266	4.815564
260.250530	7999.911067	12.043674	-0.053275	4.815569
260.487482	7999.930926	12.048679	-0.053319	4.815574
260.295479	7999.908573	12.053683	-0.053283	4.815568
260.278378	7999.945656	12.058688	-0.053280	4.815579
260.290220	7999.954380	12.063693	-0.053282	4.815582
260.374246	7999.946126	12.068698	-0.053297	4.815579
260.263843	7999.971013	12.073703	-0.053277	4.815587
260.258110	7999.903641	12.078707	-0.053275	4.815567
260.410181	7999.945610	12.083712	-0.053304	4.815578
260.289415	7999.937229	12.088717	-0.053281	4.815577
260.227445	7999.941549	12.093722	-0.053269	4.815578
260.301430	7999.942742	12.098727	-0.053283	4.815578
260.318239	7999.909904	12.103731	-0.053286	4.815568
260.171751	7999.944882	12.108736	-0.053259	4.815579
260.272812	7999.927296	12.113741	-0.053277	4.815574
260.403540	7999.921937	12.118746	-0.053302	4.815572
260.559162	7999.944744	12.123751	-0.053330	4.815577
260.319582	7999.907737	12.128755	-0.053286	4.815568
260.569138	7999.941682	12.133760	-0.053332	4.815577
260.559862	7999.928707	12.138765	-0.053330	4.815573
260.540219	7999.920902	12.143770	-0.053326	4.815571
260.576380	7999.942835	12.148775	-0.053333	4.815577
260.620302	7999.932861	12.153779	-0.053341	4.815574
260.507249	7999.951299	12.158784	-0.053320	4.815580
260.501075	7999.957594	12.163789	-0.053319	4.815582
260.431741	7999.940440	12.168794	-0.053306	4.815577
260.497538	7999.960719	12.173799	-0.053318	4.815582
260.359994	7999.925371	12.178803	-0.053292	4.815573
260.508408	7999.956603	12.183808	-0.053319	4.815581
260.348946	7999.918763	12.188813	-0.053290	4.815571
260.296467	7999.936050	12.193818	-0.053280	4.815576
260.414725	7999.960386	12.198823	-0.053302	4.815583
260.711166	7999.915012	12.203827	-0.053357	4.815568
260.339880	7999.917505	12.208832	-0.053287	4.815571
260.394396	7999.911974	12.213837	-0.053297	4.815569
260.470429	7999.919606	12.218842	-0.053312	4.815571
260.615007	7999.953980	12.223847	-0.053338	4.815580
260.440290	7999.918027	12.228851	-0.053306	4.815570
260.607615	7999.973058	12.233856	-0.053337	4.815586
260.539571	7999.931365	12.238861	-0.053324	4.815574
260.442046	7999.952191	12.243866	-0.053306	4.815580
260.488453	7999.958274	12.248871	-0.053314	4.815582
260.359341	7999.901708	12.253875	-0.053290	4.815566
260.393810	7999.935358	12.258880	-0.053296	4.815576
260.372214	7999.931793	12.263885	-0.053292	4.815575
260.475266	7999.929187	12.268890	-0.053311	4.815573
260.608250	7999.945220	12.273895	-0.053336	4.815577
260.566632	7999.913568	12.278899	-0.053328	4.815568
260.472883	7999.963285	12.283904	-0.053310	4.815583
260.489437	7999.928307	12.288909	-0.053313	4.815573
260.278871	7999.909924	12.293914	-0.053274	4.815569
260.507073	7999.929640	12.298919	-0.053316	4.815573
260.261468	7999.914958	12.303923	-0.053271	4.815570
260.324428	7999.952275	12.308928	-0.053282	4.815581
260.361105	7999.924031	12.313933	-0.053289	4.815572
260.386678	7999.931910	12.318938	-0.053293	4.815575
260.420709	7999.918572	12.323943	-0.053300	4.815571
260.319071	7999.924383	12.328947	-0.053281	4.815573
260.333795	7999.940628	12.333952	-0.053283	4.815577
260.428767	7999.933620	12.338957	-0.053301	4.815575
260.342356	7999.945017	12.343962	-0.053285	4.815579
260.246024	7999.969065	12.348967	-0.053267	4.815586
260.285594	7999.915243	12.353971	-0.053274	4.815570
260.304637	7999.940100	12.358976	-0.053277	4.815577
260.431595	7999.918664	12.363981	-0.053301	4.815571
260.245064	7999.927365	12.368986	-0.053266	4.815574
260.411135	7999.943935	12.373991	-0.053297	4.815578
260.405818	7999.922483	12.378995	-0.053296	4.815572
260.436466	7999.940055	12.384000	-0.053301	4.815577
260.577253	7999.934860	12.389005	-0.053327	4.815575
260.414456	7999.936472	12.394010	-0.053297	4.815576
260.457364	7999.976666	12.399015	-0.053305	4.815587
260.497839	7999.941010	12.404019	-0.053312	4.815577
260.565133	7999.960246	12.409024	-0.053325	4.815582
260.496937	7999.969803	12.414029	-0.053312	4.815585
260.451374	7999.934883	12.419034	-0.053303	4.815575
260.544846	7999.959883	12.424039	-0.053320	4.815582
260.532175	7999.936176	12.429043	-0.053318	4.815575
260.512372	7999.959334	12.434048	-0.053314	4.815582
260.439127	7999.936777	12.439053	-0.053300	4.815576
260.358386	7999.937588	12.444058	-0.053285	4.815577
260.403337	7999.970341	12.449063	-0.053293	4.815586
260.440018	7999.933556	12.454067	-0.053300	4.815575
260.511978	7999.944325	12.459072	-0.053313	4.815578
260.479559	7999.949126	12.464077	-0.053307	4.815579
260.395394	7999.932798	12.469082	-0.053291	4.815575
260.652603	7999.980748	12.474087	-0.053339	4.815588
260.611266	7999.951236	12.479091	-0.053331	4.815579
260.415543	7999.958719	12.484096	-0.053295	4.815582
260.551839	7999.956654	12.489101	-0.053320	4.815581
260.609593	7999.946905	12.494106	-0.053331	4.815578
260.642026	7999.978387	12.499111	-0.053337	4.815587
260.643326	7999.952771	12.504115	-0.053337	4.815580
260.688671	7999.948159	12.509120	-0.053345	4.815578
260.571894	7999.952656	12.514125	-0.053323	4.815580
260.349035	7999.928733	12.519130	-0.053282	4.815574
260.469912	7999.968060	12.524135	-0.053304	4.815585
260.585210	7999.947501	12.529139	-0.053325	4.815578
260.483335	7999.968257	12.534144	-0.053306	4.815585
260.482438	7999.941538	12.539149	-0.053306	4.815577
260.578941	7999.923877	12.544154	-0.053324	4.815572
260.631430	7999.973836	12.549159	-0.053333	4.815586
260.533669	7999.949813	12.554163	-0.053315	4.815579
260.567441	7999.927929	12.559168	-0.053321	4.815573
260.468636	7999.940192	12.564173	-0.053303	4.815577
260.207383	7999.934865	12.569178	-0.053254	4.815577
260.546638	7999.992691	12.574183	-0.053317	4.815592
260.604104	7999.923143	12.579187	-0.053328	4.815571
260.486885	7999.963936	12.584192	-0.053306	4.815584
260.617912	7999.955379	12.589197	-0.053330	4.815581
260.622827	7999.929822	12.594202	-0.053331	4.815573
260.453339	7999.979375	12.599207	-0.053299	4.815588
260.345345	7999.944507	12.604211	-0.053279	4.815579
260.453031	7999.943044	12.609216	-0.053299	4.815578
260.599031	7999.960357	12.614221	-0.053326	4.815582
260.275917	7999.957227	12.619226	-0.053266	4.815583
260.438964	7999.962003	12.624231	-0.053296	4.815583
260.462025	7999.923928	12.629235	-0.053300	4.815572
260.458996	7999.960172	12.634240	-0.053299	4.815583
260.597511	7999.937856	12.639245	-0.053325	4.815576
260.611647	7999.942346	12.644250	-0.053327	4.815577
260.575635	7999.940682	12.649255	-0.053321	4.815577
260.414010	7999.922026	12.654259	-0.053290	4.815572
260.469406	7999.927187	12.659264	-0.053301	4.815573
260.414469	7999.950841	12.664269	-0.053290	4.815580
260.337193	7999.927151	12.669274	-0.053276	4.815574
260.416418	7999.958326	12.674279	-0.053290	4.815582
260.424544	7999.928550	12.679283	-0.053292	4.815574
260.342931	7999.931483	12.684288	-0.053276	4.815575
260.364283	7999.962784	12.689293	-0.053280	4.815584
260.438466	7999.929812	12.694298	-0.053294	4.815574
260.476610	7999.938964	12.699303	-0.053301	4.815577
260.233463	7999.910441	12.704307	-0.053255	4.815569
260.450030	7999.960933	12.709312	-0.053296	4.815583
260.356969	7999.971154	12.714317	-0.053278	4.815587
260.368119	7999.930750	12.719322	-0.053280	4.815575
260.491133	7999.950892	12.724327	-0.053303	4.815580
260.690002	7999.900727	12.729331	-0.053340	4.815564
260.697642	7999.920061	12.734336	-0.053341	4.815570
260.483911	7999.930455	12.739341	-0.053301	4.815574
260.485001	7999.904836	12.744346	-0.053301	4.815567
260.778482	7999.971528	12.749351	-0.053356	4.815585
260.478342	7999.931400	12.754355	-0.053300	4.815574
260.383661	7999.925578	12.759360	-0.053282	4.815573
260.452130	7999.930952	12.764365	-0.053295	4.815574
260.449249	7999.894591	12.769370	-0.053294	4.815564
260.407467	7999.932340	12.774375	-0.053286	4.815575
260.637858	7999.940347	12.779379	-0.053329	4.815576
260.563075	7999.938052	12.784384	-0.053315	4.815576
260.477521	7999.936650	12.789389	-0.053299	4.815576
260.379954	7999.924375	12.794394	-0.053281	4.815573
260.660857	7999.947084	12.799399	-0.053333	4.815578
260.376128	7999.927494	12.804403	-0.053280	4.815574
260.311566	7999.931773	12.809408	-0.053267	4.815575
260.526621	7999.920311	12.814413	-0.053307	4.815571
260.425019	7999.885547	12.819418	-0.053288	4.815561
260.461614	7999.925639	12.824423	-0.053295	4.815573
260.439808	7999.899647	12.829427	-0.053291	4.815565
260.740220	7999.932284	12.834432	-0.053347	4.815573
260.552791	7999.935631	12.839437	-0.053312	4.815575
260.428174	7999.927187	12.844442	-0.053288	4.815573
260.644003	7999.963787	12.849447	-0.053328	4.815583
260.551500	7999.912087	12.854451	-0.053311	4.815568
260.634710	7999.919836	12.859456	-0.053326	4.815570
260.724701	7999.936238	12.864461	-0.053343	4.815575
260.626932	7999.929298	12.869466	-0.053325	4.815573
260.581272	7999.952036	12.874471	-0.053316	4.815580
260.573224	7999.917726	12.879475	-0.053314	4.815570
260.534031	7999.949110	12.884480	-0.053307	4.815579
260.568425	7999.944320	12.889485	-0.053313	4.815578
260.568026	7999.917609	12.894490	-0.053313	4.815570
260.668500	7999.948062	12.899495	-0.053332	4.815578
260.698294	7999.947468	12.904499	-0.053337	4.815578
260.790277	7999.978851	12.909504	-0.053354	4.815587
260.812785	7999.949309	12.914509	-0.053358	4.815578
260.627649	7999.925999	12.919514	-0.053324	4.815572
260.732999	7999.977887	12.924519	-0.053343	4.815587
260.700195	7999.928226	12.929523	-0.053337	4.815572
260.542921	7999.968367	12.934528	-0.053307	4.815585
260.589381	7999.981925	12.939533	-0.053316	4.815589
260.409212	7999.924529	12.944538	-0.053282	4.815573
260.559422	7999.944045	12.949543	-0.053310	4.815578
260.735982	7999.935160	12.954547	-0.053343	4.815574
260.540746	7999.945855	12.959552	-0.053306	4.815578
260.833538	7999.939929	12.964557	-0.053361	4.815575
260.849007	7999.930560	12.969562	-0.053364	4.815572
260.766066	7999.976182	12.974567	-0.053348	4.815586
260.731783	7999.914751	12.979571	-0.053342	4.815568
260.648931	7999.927274	12.984576	-0.053326	4.815572
260.661567	7999.941349	12.989581	-0.053328	4.815577
260.556840	7999.923619	12.994586	-0.053309	4.815572
260.732294	7999.976646	12.999591	-0.053341	4.815587
260.484510	7999.903202	13.004595	-0.053295	4.815566
260.414783	7999.915938	13.009600	-0.053282	4.815570
260.710857	7999.945301	13.014605	-0.053337	4.815577
260.530744	7999.901786	13.019610	-0.053303	4.815566
260.555977	7999.954505	13.024615	-0.053308	4.815581
260.447284	7999.924965	13.029619	-0.053287	4.815573
260.708138	7999.934536	13.034624	-0.053336	4.815574
260.746791	7999.940493	13.039629	-0.053343	4.815576
260.503222	7999.927978	13.044634	-0.053297	4.815573
260.822140	7999.950239	13.049639	-0.053357	4.815578
260.663815	7999.916688	13.054643	-0.053327	4.815569
260.508907	7999.947258	13.059648	-0.053298	4.815579
260.755263	7999.952322	13.064653	-0.053344	4.815579
260.765541	7999.921513	13.069658	-0.053346	4.815570
260.717075	7999.952747	13.074663	-0.053336	4.815580
260.737573	7999.928511	13.079667	-0.053340	4.815572
260.617799	7999.936162	13.084672	-0.053318	4.815575
260.866973	7999.959424	13.089677	-0.053364	4.815581
260.571467	7999.905490	13.094682	-0.053309	4.815567
260.658367	7999.951739	13.099687	-0.053325	4.815580
260.695444	7999.928840	13.104691	-0.053332	4.815573
260.564371	7999.930969	13.109696	-0.053307	4.815574
260.958601	7999.940573	13.114701	-0.053380	4.815575
260.857311	7999.936780	13.119706	-0.053361	4.815574
260.821494	7999.954338	13.124711	-0.053355	4.815580
260.793064	7999.927171	13.129715	-0.053349	4.815572
260.784611	7999.948378	13.134720	-0.053348	4.815578
260.962250	7999.983290	13.139725	-0.053381	4.815587
260.609241	7999.935894	13.144730	-0.053315	4.815575
260.698405	7999.941605	13.149735	-0.053331	4.815577
260.600030	7999.920775	13.154739	-0.053313	4.815571
260.420343	7999.934926	13.159744	-0.053279	4.815576
260.561160	7999.943612	13.164749	-0.053305	4.815578
260.634191	7999.925569	13.169754	-0.053319	4.815572
260.727124	7999.947357	13.174759	-0.053336	4.815578
260.612495	7999.921991	13.179763	-0.053314	4.815571
260.636994	7999.922379	13.184768	-0.053319	4.815571
260.797953	7999.932461	13.189773	-0.053349	4.815573
260.707893	7999.923511	13.194778	-0.053332	4.815571
260.577898	7999.947012	13.199783	-0.053307	4.815579
260.797287	7999.962315	13.204787	-0.053348	4.815582
260.649209	7999.957760	13.209792	-0.053321	4.815582
260.718688	7999.951405	13.214797	-0.053333	4.815579
260.783594	7999.926824	13.219802	-0.053345	4.815572
260.611789	7999.957119	13.224807	-0.053313	4.815582
260.766845	7999.924394	13.229811	-0.053342	4.815571
260.718394	7999.936409	13.234816	-0.053333	4.815575
260.748166	7999.972118	13.239821	-0.053338	4.815585
260.658615	7999.900179	13.244826	-0.053321	4.815565
260.748644	7999.965698	13.249831	-0.053338	4.815583
260.663869	7999.929072	13.254835	-0.053322	4.815573
260.509844	7999.954318	13.259840	-0.053293	4.815581
260.597968	7999.957876	13.264845	-0.053310	4.815582
260.440500	7999.919001	13.269850	-0.053280	4.815571
260.517909	7999.922385	13.274855	-0.053294	4.815572
260.505235	7999.914694	13.279859	-0.053292	4.815570
260.661822	7999.923636	13.284864	-0.053321	4.815572
260.812643	7999.933553	13.289869	-0.053349	4.815574
260.579990	7999.908403	13.294874	-0.053306	4.815567
260.529379	7999.953482	13.299879	-0.053296	4.815581
260.713031	7999.924426	13.304883	-0.053330	4.815572
260.607983	7999.916300	13.309888	-0.053310	4.815570
260.851353	7999.951213	13.314893	-0.053356	4.815579
260.520268	7999.920191	13.319898	-0.053294	4.815571
260.609035	7999.934437	13.324903	-0.053310	4.815575
260.492610	7999.920788	13.329907	-0.053288	4.815572
260.532637	7999.923563	13.334912	-0.053296	4.815572
260.773626	7999.934946	13.339917	-0.053340	4.815574
260.602147	7999.924672	13.344922	-0.053308	4.815572
260.615718	7999.933424	13.349927	-0.053311	4.815575
260.825291	7999.916535	13.354931	-0.053350	4.815569
260.738603	7999.924724	13.359936	-0.053333	4.815572
260.508858	7999.936993	13.364941	-0.053291	4.815576
260.545771	7999.901279	13.369946	-0.053297	4.815566
260.591302	7999.918025	13.374951	-0.053306	4.815570
260.614671	7999.911988	13.379955	-0.053310	4.815568
260.613610	7999.932247	13.384960	-0.053310	4.815574
260.676757	7999.931128	13.389965	-0.053321	4.815574
260.471730	7999.909631	13.394970	-0.053283	4.815568
260.729916	7999.940513	13.399975	-0.053331	4.815576
260.989023	7999.932971	13.404979	-0.053379	4.815573
260.856787	7999.923335	13.409984	-0.053354	4.815571
260.806595	7999.931050	13.414989	-0.053345	4.815573
260.765703	7999.931442	13.419994	-0.053337	4.815573
260.935295	7999.952342	13.424999	-0.053368	4.815579
260.836358	7999.912283	13.430003	-0.053350	4.815567
260.637702	7999.942141	13.435008	-0.053313	4.815577
260.935666	7999.948045	13.440013	-0.053368	4.815577
260.810544	7999.926779	13.445018	-0.053345	4.815572
260.640400	7999.924001	13.450023	-0.053313	4.815572
260.764346	7999.939887	13.455027	-0.053336	4.815576
260.826842	7999.952638	13.460032	-0.053347	4.815579
260.778626	7999.942233	13.465037	-0.053338	4.815577
260.813533	7999.918232	13.470042	-0.053345	4.815569
260.783457	7999.957239	13.475047	-0.053339	4.815581
260.817963	7999.957790	13.480051	-0.053345	4.815581
260.737608	7999.938320	13.485056	-0.053330	4.815576
260.613406	7999.923476	13.490061	-0.053307	4.815572
260.655330	7999.908131	13.495066	-0.053315	4.815567
260.625897	7999.942877	13.500071	-0.053309	4.815577
260.815590	7999.932071	13.505075	-0.053344	4.815573
260.660648	7999.942353	13.510080	-0.053315	4.815577
260.871201	7999.952174	13.515085	-0.053354	4.815579
260.766508	7999.902411	13.520090	-0.053335	4.815565
260.814229	7999.967242	13.525095	-0.053344	4.815584
260.760089	7999.935386	13.530099	-0.053333	4.815575
260.627055	7999.936415	13.535104	-0.053308	4.815576
260.942755	7999.950081	13.540109	-0.053367	4.815578
260.729548	7999.945534	13.545114	-0.053327	4.815578
260.605503	7999.960590	13.550119	-0.053304	4.815583
260.912670	7999.927136	13.555123	-0.053361	4.815572
260.764334	7999.928984	13.560128	-0.053333	4.815573
260.706867	7999.964342	13.565133	-0.053323	4.815583
260.543108	7999.918958	13.570138	-0.053292	4.815571
260.766160	7999.972759	13.575143	-0.053333	4.815586
260.851298	7999.938897	13.580147	-0.053349	4.815575
260.747982	7999.929732	13.585152	-0.053330	4.815573
260.706623	7999.929049	13.590157	-0.053322	4.815573
260.859490	7999.908034	13.595162	-0.053350	4.815566
260.677925	7999.949915	13.600167	-0.053316	4.815579
260.765180	7999.939579	13.605171	-0.053332	4.815576
260.735931	7999.929482	13.610176	-0.053327	4.815573
260.783644	7999.951603	13.615181	-0.053336	4.815579
260.658949	7999.920735	13.620186	-0.053312	4.815571
260.827250	7999.943748	13.625191	-0.053343	4.815577
260.852898	7999.930274	13.630195	-0.053348	4.815573
260.641270	7999.923618	13.635200	-0.053309	4.815572
260.766462	7999.957676	13.640205	-0.053332	4.815581
260.735978	7999.918730	13.645210	-0.053326	4.815570
260.722671	7999.934520	13.650215	-0.053323	4.815575
260.673670	7999.931576	13.655219	-0.053314	4.815574
260.853321	7999.945165	13.660224	-0.053347	4.815577
260.840606	7999.934270	13.665229	-0.053345	4.815574
260.801443	7999.927216	13.670234	-0.053338	4.815572
260.647074	7999.946049	13.675239	-0.053309	4.815578
260.633434	7999.929801	13.680243	-0.053306	4.815574
260.600244	7999.945266	13.685248	-0.053300	4.815578
260.778403	7999.936408	13.690253	-0.053333	4.815575
260.851134	7999.921564	13.695258	-0.053346	4.815570
260.804973	7999.937886	13.700263	-0.053337	4.815575
260.562870	7999.917922	13.705267	-0.053292	4.815571
260.702759	7999.929796	13.710272	-0.053318	4.815573
260.921190	7999.941880	13.715277	-0.053359	4.815576
260.711201	7999.945928	13.720282	-0.053320	4.815578
261.035475	7999.980021	13.725287	-0.053380	4.815587
260.832619	7999.944678	13.730291	-0.053342	4.815577
260.750317	7999.934787	13.735296	-0.053326	4.815575
260.801036	7999.981514	13.740301	-0.053336	4.815588
260.762033	7999.928549	13.745306	-0.053328	4.815573
260.702489	7999.951061	13.750311	-0.053317	4.815580
260.781298	7999.943790	13.755315	-0.053332	4.815577
260.962817	7999.925376	13.760320	-0.053365	4.815571
260.978758	7999.960861	13.765325	-0.053368	4.815581
260.659165	7999.917213	13.770330	-0.053309	4.815570
260.685756	7999.948599	13.775335	-0.053313	4.815579
260.830533	7999.941334	13.780339	-0.053340	4.815576
260.724961	7999.925725	13.785344	-0.053320	4.815572
260.876017	7999.950594	13.790349	-0.053348	4.815579
260.845480	7999.926596	13.795354	-0.053343	4.815572
260.694071	7999.975375	13.800359	-0.053314	4.815587
260.851639	7999.943759	13.805363	-0.053344	4.815577
260.923771	7999.927837	13.810368	-0.053357	4.815572
260.822264	7999.941124	13.815373	-0.053338	4.815576
260.659048	7999.927781	13.820378	-0.053307	4.815573
260.839437	7999.940314	13.825383	-0.053341	4.815576
260.850635	7999.930876	13.830387	-0.053343	4.815573
260.713623	7999.923298	13.835392	-0.053317	4.815572
260.798297	7999.939613	13.840397	-0.053333	4.815576
260.749688	7999.921727	13.845402	-0.053324	4.815571
260.617620	7999.961211	13.850407	-0.053299	4.815583
260.492269	7999.937807	13.855411	-0.053275	4.815577
260.586553	7999.940397	13.860416	-0.053293	4.815577
260.738567	7999.931113	13.865421	-0.053321	4.815574
260.699221	7999.901633	13.870426	-0.053314	4.815565
260.766687	7999.946498	13.875431	-0.053326	4.815578
260.937937	7999.942866	13.880435	-0.053358	4.815576
260.781068	7999.934965	13.885440	-0.053328	4.815575
260.914198	7999.946729	13.890445	-0.053353	4.815577
260.823722	7999.906808	13.895450	-0.053336	4.815566
260.762270	7999.958117	13.900455	-0.053325	4.815582
260.624217	7999.918490	13.905459	-0.053299	4.815571
260.569423	7999.916521	13.910464	-0.053288	4.815570
260.676839	7999.947086	13.915469	-0.053308	4.815579
260.682996	7999.903398	13.920474	-0.053309	4.815566
260.519473	7999.925286	13.925479	-0.053279	4.815573
260.706681	7999.913371	13.930483	-0.053313	4.815569
260.803161	7999.917065	13.935488	-0.053331	4.815569
260.968105	7999.933618	13.940493	-0.053362	4.815573
260.981295	7999.931686	13.945498	-0.053364	4.815573
260.878171	7999.942811	13.950503	-0.053345	4.815577
260.814203	7999.919337	13.955507	-0.053333	4.815570
260.718028	7999.906017	13.960512	-0.053315	4.815567
260.859350	7999.942473	13.965517	-0.053341	4.815577
260.862525	7999.927565	13.970522	-0.053342	4.815572
260.853523	7999.948763	13.975527	-0.053340	4.815578
260.971106	7999.941055	13.980531	-0.053362	4.815576
260.859868	7999.912541	13.985536	-0.053341	4.815568
260.793461	7999.942415	13.990541	-0.053328	4.815577
260.815224	7999.908590	13.995546	-0.053332	4.815567
261.015879	7999.947079	14.000551	-0.053369	4.815577
260.802058	7999.960675	14.005555	-0.053329	4.815582
260.789612	7999.917751	14.010560	-0.053327	4.815570
260.901140	7999.948384	14.015565	-0.053348	4.815578
260.685152	7999.907489	14.020570	-0.053307	4.815567
260.510930	7999.939881	14.025575	-0.053275	4.815577
260.619689	7999.923487	14.030579	-0.053295	4.815572
260.584362	7999.913292	14.035584	-0.053288	4.815569
260.727346	7999.939097	14.040589	-0.053315	4.815576
260.593055	7999.925157	14.045594	-0.053290	4.815573
260.891049	7999.922519	14.050599	-0.053345	4.815571
260.719641	7999.921856	14.055603	-0.053313	4.815571
260.517017	7999.917482	14.060608	-0.053275	4.815571
260.688686	7999.936279	14.065613	-0.053307	4.815576
260.731082	7999.928416	14.070618	-0.053315	4.815573
260.608048	7999.961640	14.075623	-0.053292	4.815583
260.859075	7999.942221	14.080627	-0.053338	4.815577
260.756062	7999.921316	14.085632	-0.053319	4.815571
260.674330	7999.928518	14.090637	-0.053304	4.815573
260.621148	7999.907355	14.095642	-0.053294	4.815567
260.611378	7999.938150	14.100647	-0.053292	4.815577
260.802990	7999.940188	14.105651	-0.053327	4.815576
260.662924	7999.929357	14.110656	-0.053301	4.815574
261.097562	7999.988736	14.115661	-0.053382	4.815589
260.927860	7999.949661	14.120666	-0.053350	4.815578
260.761496	7999.952283	14.125671	-0.053319	4.815580
260.806485	7999.951936	14.130675	-0.053327	4.815580
260.840520	7999.937531	14.135680	-0.053333	4.815575
260.808804	7999.965833	14.140685	-0.053327	4.815584
260.868044	7999.913398	14.145690	-0.053338	4.815568
260.748240	7999.944540	14.150695	-0.053316	4.815578
260.780242	7999.926897	14.155699	-0.053322	4.815572
260.533810	7999.931421	14.160704	-0.053276	4.815575
260.820016	7999.965962	14.165709	-0.053329	4.815584
260.970073	7999.954511	14.170714	-0.053357	4.815580
260.725964	7999.961208	14.175719	-0.053311	4.815583
260.784935	7999.933327	14.180723	-0.053322	4.815574
260.764465	7999.914831	14.185728	-0.053318	4.815569
260.687874	7999.919981	14.190733	-0.053304	4.815571
260.655949	7999.895961	14.195738	-0.053298	4.815564
260.857823	7999.907775	14.200743	-0.053335	4.815567
260.661794	7999.943016	14.205747	-0.053298	4.815578
260.486864	7999.930550	14.210752	-0.053266	4.815575
260.773017	7999.950142	14.215757	-0.053319	4.815579
260.776375	7999.905340	14.220762	-0.053319	4.815566
260.744267	7999.918688	14.225767	-0.053313	4.815570
260.719931	7999.919349	14.230771	-0.053309	4.815571
260.917531	7999.887316	14.235776	-0.053345	4.815560
260.834706	7999.937211	14.240781	-0.053330	4.815575
260.586653	7999.903269	14.245786	-0.053283	4.815567
260.595255	7999.932227	14.250791	-0.053285	4.815575
260.623264	7999.970043	14.255795	-0.053290	4.815586
260.624368	7999.012305	14.260800	-0.053289	4.815306

260.560559	7995.919525	14.265805	-0.053275	4.814402
260.571999	7990.526574	14.270810	-0.053274	4.812824
260.448104	7983.852085	14.275815	-0.053246	4.810872
260.565512	7976.641420	14.280819	-0.053263	4.808760
260.421975	7968.976898	14.285824	-0.053232	4.806516
260.436238	7961.183150	14.290829	-0.053229	4.804232
260.326766	7953.351844	14.295834	-0.053203	4.801937
260.437322	7945.359478	14.300839	-0.053219	4.799592
260.547985	7937.463526	14.305843	-0.053234	4.797275
260.445250	7929.376881	14.310848	-0.053209	4.794901
260.357075	7921.411387	14.315853	-0.053188	4.792562
260.516335	7913.373672	14.320858	-0.053212	4.790199
260.332193	7905.439107	14.325863	-0.053172	4.787867
260.336075	7897.377385	14.330867	-0.053168	4.785496
260.237925	7889.425394	14.335872	-0.053144	4.783156
260.438302	7881.346718	14.340877	-0.053176	4.780776
260.280971	7873.431494	14.345882	-0.053142	4.778445
260.324677	7865.354442	14.350887	-0.053144	4.776064
260.399052	7857.369653	14.355891	-0.053153	4.773709
260.264931	7849.327967	14.360896	-0.053123	4.771337
260.145806	7841.387807	14.365901	-0.053095	4.768994
260.082224	7833.446998	14.370906	-0.053078	4.766649
260.103467	7825.343195	14.375911	-0.053076	4.764254
259.908756	7817.441510	14.380915	-0.053035	4.761919
260.018860	7809.323618	14.385920	-0.053050	4.759518
260.103592	7801.456309	14.390925	-0.053061	4.757189
259.998839	7793.347168	14.395930	-0.053036	4.754789
259.935680	7785.300584	14.400935	-0.053019	4.752405
260.205025	7777.330142	14.405939	-0.053063	4.750042
259.680456	7769.322459	14.410944	-0.052960	4.747670
259.740892	7761.323020	14.415949	-0.052966	4.745296
259.847885	7753.360647	14.420954	-0.052981	4.742933
259.743662	7745.309688	14.425959	-0.052956	4.740542
259.717945	7737.373921	14.430963	-0.052946	4.738184
259.666494	7729.290673	14.435968	-0.052931	4.735782
259.676913	7721.307646	14.440973	-0.052928	4.733407
259.561265	7713.309622	14.445978	-0.052901	4.731028
259.555004	7705.309335	14.450983	-0.052894	4.728646
259.659520	7697.350756	14.455987	-0.052908	4.726275
259.681061	7689.326289	14.460992	-0.052907	4.723884
259.553510	7681.316126	14.465997	-0.052878	4.721496
259.497490	7673.310671	14.471002	-0.052862	4.719108
259.335177	7665.322026	14.476007	-0.052827	4.716724
259.683361	7657.326927	14.481011	-0.052886	4.714335
259.409736	7649.261970	14.486016	-0.052830	4.711926
259.454883	7641.274670	14.491021	-0.052833	4.709539
259.523132	7633.363593	14.496026	-0.052840	4.707172
259.465243	7625.285545	14.501031	-0.052824	4.704755
259.402301	7617.349260	14.506035	-0.052807	4.702380
259.390089	7609.260020	14.511040	-0.052799	4.699957
259.193256	7601.336214	14.516045	-0.052758	4.697582
259.193772	7593.285566	14.521050	-0.052752	4.695168
259.217789	7585.317243	14.526055	-0.052751	4.692778
259.154152	7577.309817	14.531059	-0.052734	4.690375
259.153363	7569.258046	14.536064	-0.052729	4.687957
259.353032	7561.277015	14.541069	-0.052761	4.685558
258.980038	7553.316606	14.546074	-0.052686	4.683166
259.076416	7545.295433	14.551079	-0.052698	4.680753
259.194852	7537.297150	14.556083	-0.052715	4.678346
259.041983	7529.304733	14.561088	-0.052681	4.675940
259.105965	7521.242912	14.566093	-0.052688	4.673511
259.090659	7513.162127	14.571098	-0.052680	4.671076
259.071537	7505.191129	14.576103	-0.052671	4.668672
258.969632	7497.218741	14.581107	-0.052646	4.666267
258.726983	7489.203434	14.586112	-0.052596	4.663848
258.713057	7481.214938	14.591117	-0.052588	4.661435
258.662203	7473.260416	14.596122	-0.052573	4.659031
258.703986	7465.253555	14.601127	-0.052576	4.656611
258.722466	7457.228078	14.606131	-0.052574	4.654183
258.486857	7449.199856	14.611136	-0.052525	4.651753
258.637541	7441.187295	14.616141	-0.052547	4.649327
258.755802	7433.261201	14.621146	-0.052564	4.646926
258.489491	7425.195138	14.626151	-0.052509	4.644481
258.413367	7417.274834	14.631155	-0.052490	4.642079
258.454664	7409.174783	14.636160	-0.052492	4.639621
258.557269	7401.268285	14.641165	-0.052506	4.637220
258.320185	7393.205022	14.646170	-0.052456	4.634771
258.152040	7385.153406	14.651175	-0.052419	4.632324
258.294949	7377.169100	14.656179	-0.052441	4.629896
258.151570	7369.212246	14.661184	-0.052409	4.627475
258.116378	7361.146920	14.666189	-0.052397	4.625020
258.196663	7353.202795	14.671194	-0.052406	4.622601
258.075981	7345.168492	14.676199	-0.052379	4.620152
258.045922	7337.246013	14.681203	-0.052368	4.617737
257.954928	7329.180362	14.686208	-0.052345	4.615276
258.135812	7321.184458	14.691213	-0.052374	4.612836
257.895913	7313.169368	14.696218	-0.052324	4.610388
257.742440	7305.162675	14.701223	-0.052290	4.607942
257.928641	7297.189657	14.706227	-0.052319	4.605504
257.900310	7289.169975	14.711232	-0.052309	4.603051
257.749909	7281.153707	14.716237	-0.052275	4.600598
257.806318	7273.227132	14.721242	-0.052280	4.598171
257.938909	7265.158925	14.726247	-0.052300	4.595699
257.822314	7257.147373	14.731251	-0.052273	4.593244
257.691658	7249.081160	14.736256	-0.052243	4.590770
257.945448	7241.116194	14.741261	-0.052285	4.588326
257.684681	7233.112847	14.746266	-0.052231	4.585869
257.478118	7225.116814	14.751271	-0.052187	4.583412
257.513276	7217.169190	14.756275	-0.052188	4.580970
257.534374	7209.136524	14.761280	-0.052187	4.578499
257.474754	7201.149017	14.766285	-0.052171	4.576042
257.536689	7193.148201	14.771290	-0.052177	4.573579
257.569688	7185.106179	14.776295	-0.052178	4.571102
257.512800	7177.153914	14.781299	-0.052162	4.568651
257.486054	7169.115742	14.786304	-0.052151	4.566173
257.425836	7161.156954	14.791309	-0.052135	4.563717
257.428505	7153.142557	14.796314	-0.052130	4.561243
257.406848	7145.139698	14.801319	-0.052121	4.558771
257.323812	7137.165720	14.806323	-0.052100	4.556307
257.313987	7129.128110	14.811328	-0.052093	4.553822
257.102302	7121.083803	14.816333	-0.052048	4.551333
257.146262	7113.106186	14.821338	-0.052051	4.548864
257.226680	7105.101453	14.826343	-0.052060	4.546385
257.359427	7097.130989	14.831347	-0.052080	4.543916
257.249194	7089.127963	14.836352	-0.052054	4.541434
257.232989	7081.131820	14.841357	-0.052046	4.538954
257.219017	7073.149100	14.846362	-0.052038	4.536476
256.997309	7065.071569	14.851367	-0.051991	4.533967
257.004139	7057.125684	14.856371	-0.051987	4.531499
256.916298	7049.087389	14.861376	-0.051965	4.528999
257.104158	7041.126917	14.866381	-0.051995	4.526524
257.017109	7033.079430	14.871386	-0.051973	4.524019
256.828425	7025.110356	14.876391	-0.051933	4.521537
257.111481	7017.152209	14.881395	-0.051980	4.519058
256.877276	7009.157263	14.886400	-0.051931	4.516565
256.862554	7001.089047	14.891405	-0.051923	4.514048
256.796297	6993.036764	14.896410	-0.051905	4.511535
256.390432	6985.006813	14.901415	-0.051825	4.509027
256.571371	6977.032457	14.906419	-0.051853	4.506536
256.568155	6969.023113	14.911424	-0.051847	4.504032
256.624466	6961.124474	14.916429	-0.051852	4.501561
256.670388	6953.072678	14.921434	-0.051855	4.499042
256.659449	6945.076744	14.926439	-0.051848	4.496538
256.708575	6937.082717	14.931443	-0.051852	4.494033
256.546393	6929.026476	14.936448	-0.051816	4.491507
256.439423	6921.056886	14.941453	-0.051791	4.489007
256.370725	6913.103336	14.946458	-0.051773	4.486511
256.358089	6905.015517	14.951463	-0.051765	4.483971
256.406022	6897.130338	14.956467	-0.051769	4.481494
256.441333	6889.093768	14.961472	-0.051770	4.478967
256.377752	6881.115387	14.966477	-0.051753	4.476458
256.358417	6873.100367	14.971482	-0.051744	4.473935
256.350140	6865.032273	14.976487	-0.051737	4.471394
256.363178	6857.079479	14.981491	-0.051734	4.468889
256.276403	6849.013502	14.986496	-0.051713	4.466346
256.302846	6841.018111	14.991501	-0.051712	4.463824
256.175974	6833.045884	14.996506	-0.051683	4.461307
255.934302	6825.036125	15.001511	-0.051633	4.458777
256.152289	6817.023358	15.006515	-0.051668	4.456246
256.070367	6809.045486	15.011520	-0.051648	4.453723
255.993925	6800.999093	15.016525	-0.051628	4.451177
255.991408	6793.029355	15.021530	-0.051622	4.448655
255.945007	6784.970114	15.026535	-0.051608	4.446102
256.134757	6777.038454	15.031539	-0.051638	4.443590
255.953797	6769.025662	15.036544	-0.051599	4.441048
255.867992	6761.041811	15.041549	-0.051578	4.438515
256.041612	6753.025521	15.046554	-0.051605	4.435971
255.888266	6744.989882	15.051559	-0.051571	4.433418
255.954534	6736.963658	15.056563	-0.051578	4.430868
255.635265	6728.960384	15.061568	-0.051513	4.428322
255.808799	6720.976194	15.066573	-0.051540	4.425782
255.699983	6713.039943	15.071578	-0.051515	4.423255
255.552271	6704.981484	15.076583	-0.051482	4.420688
255.555919	6697.001847	15.081587	-0.051477	4.418145
255.352286	6688.977165	15.086592	-0.051434	4.415585
255.348929	6680.985392	15.091597	-0.051428	4.413035
255.434351	6672.973379	15.096602	-0.051438	4.410477
255.419571	6664.966618	15.101607	-0.051430	4.407919
255.420454	6656.975982	15.106611	-0.051425	4.405365
255.259900	6649.023869	15.111616	-0.051390	4.402821
255.282040	6641.000238	15.116621	-0.051389	4.400253
255.357456	6633.070071	15.121626	-0.051397	4.397715
255.260963	6624.988595	15.126631	-0.051374	4.395125
255.451212	6616.981964	15.131635	-0.051404	4.392559
255.136744	6608.924503	15.136640	-0.051340	4.389973
255.048485	6600.990474	15.141645	-0.051319	4.387426
255.208402	6592.967269	15.146650	-0.051343	4.384850
255.213766	6585.066116	15.151655	-0.051339	4.382312
255.167123	6577.023909	15.156659	-0.051325	4.379726
255.070345	6569.038819	15.161664	-0.051301	4.377156
255.040363	6560.989353	15.166669	-0.051290	4.374565
254.882607	6553.023626	15.171674	-0.051256	4.371998
254.860943	6544.955476	15.176679	-0.051246	4.369398
255.110315	6537.025366	15.181683	-0.051287	4.366842
254.987480	6528.985121	15.186688	-0.051259	4.364247
254.872378	6521.025936	15.191693	-0.051232	4.361677
254.755875	6513.025149	15.196698	-0.051205	4.359092
254.757282	6505.012332	15.201703	-0.051200	4.356502
254.768843	6496.972239	15.206707	-0.051197	4.353901
254.727669	6488.857012	15.211712	-0.051184	4.351275
254.744567	6480.871782	15.216717	-0.051182	4.348689
254.745737	6472.926306	15.221722	-0.051177	4.346115
254.620530	6464.957379	15.226727	-0.051148	4.343530
254.743802	6456.962038	15.231731	-0.051166	4.340937
254.581764	6448.999617	15.236736	-0.051130	4.338352
254.488712	6440.990565	15.241741	-0.051108	4.335750
254.679698	6432.937959	15.246746	-0.051138	4.333134
254.349254	6424.938971	15.251751	-0.051071	4.330531
254.357949	6416.984461	15.256755	-0.051067	4.327943
254.275504	6408.931289	15.261760	-0.051046	4.325320
254.303366	6400.964878	15.266765	-0.051046	4.322725
254.296916	6393.018386	15.271770	-0.051040	4.320135
254.140326	6384.981535	15.276775	-0.051005	4.317512
254.460822	6376.977871	15.281779	-0.051060	4.314903
254.388213	6368.928792	15.286784	-0.051041	4.312274
254.154257	6360.870287	15.291789	-0.050992	4.309639
254.195304	6352.968785	15.296794	-0.050994	4.307056
254.123230	6344.939237	15.301799	-0.050975	4.304428
254.023813	6336.997277	15.306803	-0.050952	4.301828
253.951090	6328.966146	15.311808	-0.050933	4.299196
253.908684	6320.918281	15.316813	-0.050919	4.296558
254.011881	6312.925101	15.321818	-0.050933	4.293938
253.920805	6304.890218	15.326823	-0.050911	4.291300
253.859797	6296.925153	15.331827	-0.050894	4.288684
253.794440	6288.952741	15.336832	-0.050877	4.286064
253.727848	6280.958689	15.341837	-0.050859	4.283435
253.693066	6272.970664	15.346842	-0.050847	4.280807
253.688354	6264.946971	15.351847	-0.050841	4.278166
253.896028	6256.969170	15.356851	-0.050874	4.275540
253.786012	6248.896533	15.361856	-0.050849	4.272879
253.936652	6240.851461	15.366861	-0.050871	4.270227
253.792215	6232.920352	15.371866	-0.050839	4.267609
253.539241	6224.860963	15.376871	-0.050787	4.264945
253.685269	6216.935797	15.381875	-0.050808	4.262328
253.703379	6208.896185	15.386880	-0.050807	4.259670
253.526865	6200.967848	15.391885	-0.050768	4.257046
253.408650	6192.932563	15.396890	-0.050741	4.254385
253.621530	6184.874359	15.401895	-0.050775	4.251718
253.465324	6176.892622	15.406899	-0.050741	4.249071
253.300587	6168.915227	15.411904	-0.050705	4.246424
253.403616	6160.917451	15.416909	-0.050719	4.243771
253.553763	6152.983458	15.421914	-0.050741	4.241138
253.362390	6144.951394	15.426919	-0.050700	4.238467
253.259434	6136.980133	15.431923	-0.050676	4.235816
253.294491	6128.918908	15.436928	-0.050677	4.233134
253.218048	6120.887605	15.441933	-0.050657	4.230460
253.395757	6112.930779	15.446938	-0.050685	4.227811
253.212008	6104.898742	15.451943	-0.050646	4.225132
253.217698	6096.957010	15.456947	-0.050641	4.222484
252.997782	6088.928836	15.461952	-0.050595	4.219802
253.006990	6080.962502	15.466957	-0.050591	4.217142
252.987745	6072.974042	15.471962	-0.050583	4.214472
252.816551	6064.925299	15.476967	-0.050545	4.211779
252.762288	6056.911766	15.481971	-0.050530	4.209097
252.893922	6048.960075	15.486976	-0.050549	4.206437
252.709093	6040.944969	15.491981	-0.050509	4.203749
252.645953	6032.982464	15.496986	-0.050492	4.201080
252.616847	6024.967226	15.501991	-0.050481	4.198391
252.636061	6016.978856	15.506995	-0.050480	4.195709
252.784469	6008.867884	15.512000	-0.050502	4.192987
252.561162	6000.820493	15.517005	-0.050455	4.190280
252.746722	5992.896044	15.522010	-0.050484	4.187617
252.590843	5984.857824	15.527015	-0.050450	4.184910
252.436807	5976.922132	15.532019	-0.050416	4.182236
252.514966	5968.926525	15.537024	-0.050425	4.179542
252.568599	5960.924827	15.542029	-0.050430	4.176845
252.648422	5952.932963	15.547034	-0.050439	4.174149
252.434300	5944.873798	15.552039	-0.050394	4.171426
252.522347	5936.904975	15.557043	-0.050405	4.168735
252.397421	5928.945709	15.562048	-0.050377	4.166043
252.072845	5920.939395	15.567053	-0.050311	4.163331
252.132365	5912.947418	15.572058	-0.050317	4.160626
252.056823	5904.943158	15.577063	-0.050297	4.157914
251.933883	5896.947641	15.582067	-0.050269	4.155203
252.025659	5888.871709	15.587072	-0.050281	4.152465
252.103303	5880.851226	15.592077	-0.050290	4.149744
251.897327	5872.904780	15.597082	-0.050246	4.147042
251.880722	5864.888022	15.602087	-0.050238	4.144318
251.948956	5856.913912	15.607091	-0.050245	4.141607
251.997797	5848.926437	15.612096	-0.050249	4.138890
252.025434	5840.911962	15.617101	-0.050249	4.136161
252.306137	5832.900030	15.622106	-0.050296	4.133434
252.108256	5824.871319	15.627111	-0.050253	4.130695
251.871959	5816.957369	15.632115	-0.050204	4.127992
251.931966	5808.886070	15.637120	-0.050210	4.125237
251.905998	5800.924724	15.642125	-0.050200	4.122517
251.713020	5792.947465	15.647130	-0.050158	4.119787
251.676137	5784.990737	15.652135	-0.050146	4.117065
251.807048	5776.916299	15.657139	-0.050165	4.114302
251.616360	5768.838412	15.662144	-0.050124	4.111533
251.506009	5760.884103	15.667149	-0.050099	4.108805
251.507288	5752.899940	15.672154	-0.050093	4.106066
251.421414	5744.913538	15.677159	-0.050072	4.103324
251.347938	5736.940219	15.682163	-0.050053	4.100584
251.483634	5728.943289	15.687168	-0.050073	4.097837
251.412045	5720.909823	15.692173	-0.050054	4.095074
251.330284	5712.938438	15.697178	-0.050034	4.092329
251.219407	5704.894745	15.702183	-0.050008	4.089557
251.416850	5696.935858	15.707187	-0.050039	4.086817
251.256837	5688.933964	15.712192	-0.050004	4.084055
251.125501	5680.964450	15.717197	-0.049974	4.081303
251.147535	5672.978869	15.722202	-0.049973	4.078546
251.194709	5664.958840	15.727207	-0.049977	4.075775
251.076768	5656.979808	15.732211	-0.049949	4.073014
250.975197	5648.927112	15.737216	-0.049925	4.070226
250.969729	5640.947262	15.742221	-0.049919	4.067463
250.951625	5632.947244	15.747226	-0.049910	4.064691
250.908972	5624.940210	15.752231	-0.049897	4.061914
251.250101	5616.917394	15.757235	-0.049955	4.059135
251.162238	5608.960023	15.762240	-0.049933	4.056371
251.049209	5600.917554	15.767245	-0.049907	4.053575
251.097381	5592.926880	15.772250	-0.049910	4.050797
251.147395	5584.933525	15.777255	-0.049914	4.048016
251.019243	5576.960366	15.782259	-0.049885	4.045239
251.059823	5569.005271	15.787264	-0.049887	4.042467
251.008651	5560.939597	15.792269	-0.049873	4.039655
250.847126	5553.017588	15.797274	-0.049837	4.036888
250.625249	5544.906141	15.802279	-0.049790	4.034053
250.789144	5536.846309	15.807283	-0.049816	4.031239
251.009165	5528.866366	15.812288	-0.049851	4.028452
250.600908	5520.883646	15.817293	-0.049770	4.025653
250.751449	5512.948974	15.822298	-0.049793	4.022878
250.626660	5504.898251	15.827303	-0.049764	4.020055
250.518523	5496.970002	15.832307	-0.049739	4.017274
250.521121	5488.953418	15.837312	-0.049734	4.014461
250.279136	5480.913387	15.842317	-0.049683	4.011634
250.309470	5472.929090	15.847322	-0.049684	4.008829
250.072220	5464.905626	15.852327	-0.049634	4.006005
250.345914	5456.957938	15.857331	-0.049680	4.003213
250.243482	5448.941486	15.862336	-0.049655	4.000388
250.146302	5440.966822	15.867341	-0.049632	3.997577
250.387084	5432.930985	15.872346	-0.049671	3.994748
250.368750	5424.884372	15.877351	-0.049663	3.991908
250.359921	5416.906700	15.882355	-0.049656	3.989091
250.254255	5408.916205	15.887360	-0.049631	3.986266
250.365522	5400.915135	15.892365	-0.049646	3.983439
250.213986	5392.961115	15.897370	-0.049612	3.980622
250.069405	5384.958704	15.902375	-0.049580	3.977786
250.069515	5376.971975	15.907379	-0.049575	3.974956
249.936147	5368.947100	15.912384	-0.049545	3.972108
249.939197	5360.913637	15.917389	-0.049540	3.969257
250.044910	5352.972447	15.922394	-0.049554	3.966439
250.033606	5344.960802	15.927399	-0.049547	3.963592
249.987041	5336.963646	15.932403	-0.049533	3.960747
249.902307	5329.003047	15.937408	-0.049512	3.957912
249.729966	5320.990228	15.942413	-0.049474	3.955056
249.836592	5312.953043	15.947418	-0.049489	3.952193
249.530566	5304.946212	15.952423	-0.049427	3.949332
249.661540	5296.950957	15.957427	-0.049446	3.946481
249.636051	5288.987498	15.962432	-0.049436	3.943636
249.520882	5280.994953	15.967437	-0.049409	3.940777
249.511475	5273.047504	15.972442	-0.049402	3.937934
249.381186	5264.966235	15.977447	-0.049372	3.935039
249.515376	5256.980531	15.982451	-0.049392	3.932181
249.324997	5248.986436	15.987456	-0.049351	3.929312
249.409053	5241.020081	15.992461	-0.049361	3.926456
249.450923	5233.025990	15.997466	-0.049364	3.923587
249.278751	5225.032120	16.002471	-0.049326	3.920712
249.386508	5217.053336	16.007475	-0.049341	3.917845
249.365753	5209.017548	16.012480	-0.049332	3.914953
249.395756	5200.978168	16.017485	-0.049332	3.912059
249.407694	5192.980308	16.022490	-0.049329	3.909178
249.360609	5185.004391	16.027495	-0.049315	3.906301
249.328848	5177.021471	16.032499	-0.049304	3.903419
249.172367	5169.020732	16.037504	-0.049269	3.900527
248.970646	5161.033554	16.042509	-0.049226	3.897637
249.067261	5153.027206	16.047514	-0.049239	3.894743
248.957895	5145.008334	16.052519	-0.049213	3.891839
249.177428	5136.988410	16.057523	-0.049249	3.888938
249.105768	5128.997621	16.062528	-0.049230	3.886040
248.928522	5121.031372	16.067533	-0.049192	3.883147
248.905926	5113.042224	16.072538	-0.049182	3.880246
248.875749	5105.033703	16.077543	-0.049171	3.877336
248.789231	5096.999061	16.082547	-0.049150	3.874413
248.821831	5088.756502	16.087552	-0.049150	3.871415
248.660736	5080.853968	16.092557	-0.049115	3.868534
248.797466	5072.906036	16.097562	-0.049135	3.865641
248.627910	5064.973068	16.102567	-0.049098	3.862745
248.661873	5056.999887	16.107571	-0.049099	3.859836
248.910802	5049.024277	16.112576	-0.049140	3.856928
248.730412	5041.005754	16.117581	-0.049101	3.853993
248.647252	5033.029832	16.122586	-0.049081	3.851074
248.534474	5025.005381	16.127591	-0.049054	3.848135
248.758157	5017.019423	16.132595	-0.049091	3.845214
248.573595	5009.077667	16.137600	-0.049051	3.842298
248.373663	5001.051024	16.142605	-0.049008	3.839349
248.537211	4993.112957	16.147610	-0.049034	3.836438
248.522964	4985.043997	16.152615	-0.049026	3.833473
248.287736	4977.056661	16.157619	-0.048976	3.830531
248.153953	4969.068085	16.162624	-0.048946	3.827588
248.176738	4961.017439	16.167629	-0.048945	3.824623
248.135289	4953.107958	16.172634	-0.048932	3.821707
248.038488	4945.114666	16.177639	-0.048909	3.818756
248.087859	4937.095477	16.182643	-0.048913	3.815797
248.204303	4929.067621	16.187648	-0.048929	3.812834
248.141768	4921.044566	16.192653	-0.048912	3.809866
248.192664	4913.106354	16.197658	-0.048916	3.806930
247.979687	4905.079316	16.202663	-0.048871	3.803952
247.971144	4897.146849	16.207667	-0.048864	3.801012
247.930793	4889.155933	16.212672	-0.048851	3.798048
248.195060	4881.094397	16.217677	-0.048895	3.795061
248.140317	4873.090807	16.222682	-0.048880	3.792087
247.755394	4865.080458	16.227687	-0.048803	3.789100
247.803387	4857.065822	16.232691	-0.048806	3.786119
247.761399	4849.115681	16.237696	-0.048793	3.783158
247.625794	4841.093675	16.242701	-0.048762	3.780166
247.868205	4833.131423	16.247706	-0.048802	3.777202
247.853504	4825.102258	16.252711	-0.048794	3.774205
247.813203	4817.104431	16.257715	-0.048781	3.771216
247.767990	4809.117442	16.262720	-0.048768	3.768229
247.631878	4801.075636	16.267725	-0.048737	3.765218
247.773056	4793.166687	16.272730	-0.048758	3.762260
247.684779	4785.118115	16.277735	-0.048736	3.759242
247.758487	4777.144279	16.282739	-0.048744	3.756253
247.755850	4769.119128	16.287744	-0.048739	3.753241
247.581442	4761.090322	16.292749	-0.048701	3.750221
247.466726	4753.163135	16.297754	-0.048674	3.747238
247.539896	4745.126064	16.302759	-0.048682	3.744216
247.561672	4737.176585	16.307763	-0.048681	3.741223
247.483824	4729.172647	16.312768	-0.048661	3.738205
247.331424	4721.158400	16.317773	-0.048628	3.735179
247.241933	4713.164932	16.322778	-0.048606	3.732160
247.249499	4705.136298	16.327783	-0.048602	3.729127
247.369678	4697.163988	16.332787	-0.048619	3.726116
247.356847	4689.191721	16.337792	-0.048611	3.723099
247.093665	4681.219703	16.342797	-0.048557	3.720074
247.146550	4673.252113	16.347802	-0.048561	3.717055
247.062712	4665.185419	16.352807	-0.048540	3.713994
247.007203	4657.116192	16.357811	-0.048525	3.710929
246.942926	4649.156905	16.362816	-0.048507	3.707904
247.161238	4641.096324	16.367821	-0.048543	3.704844
246.824912	4633.228534	16.372826	-0.048475	3.701842
246.583533	4625.247180	16.377831	-0.048424	3.698796
246.887331	4617.223667	16.382835	-0.048476	3.695745
246.703883	4609.225605	16.387840	-0.048436	3.692689
246.681580	4601.190112	16.392845	-0.048427	3.689621
246.696708	4593.276445	16.397850	-0.048424	3.686597
246.719760	4585.254504	16.402855	-0.048423	3.683530
246.620348	4577.266142	16.407859	-0.048399	3.680469
246.643946	4569.282783	16.412864	-0.048398	3.677412
246.704632	4561.227067	16.417869	-0.048404	3.674325
246.711324	4553.253291	16.422874	-0.048400	3.671265
246.385877	4545.263829	16.427879	-0.048334	3.668188
246.541326	4537.252008	16.432883	-0.048358	3.665113
246.631192	4529.295094	16.437888	-0.048369	3.662054
246.520196	4521.255492	16.442893	-0.048343	3.658956
246.274404	4513.299959	16.447898	-0.048292	3.655884
246.472958	4505.248067	16.452903	-0.048324	3.652784
246.714479	4497.225858	16.457907	-0.048363	3.649694
246.524985	4489.293250	16.462912	-0.048323	3.646624
246.236720	4481.287044	16.467917	-0.048264	3.643521
246.473835	4473.318452	16.472922	-0.048303	3.640443
246.251538	4465.311762	16.477927	-0.048256	3.637336
246.198158	4457.315586	16.482931	-0.048241	3.634235
246.008970	4449.295504	16.487936	-0.048200	3.631119
246.001968	4441.267267	16.492941	-0.048193	3.628001
246.156493	4433.272371	16.497946	-0.048217	3.624898
246.165383	4425.314539	16.502951	-0.048213	3.621803
246.013124	4417.342794	16.507955	-0.048179	3.618695
245.694522	4409.358477	16.512960	-0.048115	3.615575
245.759793	4401.325221	16.517965	-0.048122	3.612444
245.927768	4393.334790	16.522970	-0.048148	3.609330
245.908125	4385.325397	16.527975	-0.048139	3.606201
245.768182	4377.360290	16.532979	-0.048107	3.603082
245.806705	4369.379009	16.537984	-0.048109	3.599960
245.724025	4361.415728	16.542989	-0.048088	3.596839
245.587858	4353.434593	16.547994	-0.048058	3.593706
245.545539	4345.369409	16.552999	-0.048044	3.590540
245.571466	4337.386684	16.558003	-0.048044	3.587406
245.590840	4329.405054	16.563008	-0.048042	3.584270
245.498140	4321.422693	16.568013	-0.048020	3.581127
245.638214	4313.439926	16.573018	-0.048040	3.577987
245.397607	4305.432548	16.578023	-0.047990	3.574825
245.539233	4297.432835	16.583027	-0.048011	3.571673
245.634381	4289.426151	16.588032	-0.048024	3.568515
245.457825	4281.412579	16.593037	-0.047985	3.565344
245.470269	4273.479844	16.598042	-0.047982	3.562207
245.464382	4265.462430	16.603047	-0.047976	3.559033
245.389044	4257.489627	16.608051	-0.047957	3.555872
245.433500	4249.430045	16.613056	-0.047960	3.552677
245.074249	4241.375601	16.618061	-0.047887	3.549469
245.290684	4233.394705	16.623066	-0.047922	3.546305
244.969169	4225.419613	16.628071	-0.047857	3.543125
244.896740	4217.446423	16.633075	-0.047838	3.539949
245.026789	4209.491007	16.638080	-0.047857	3.536784
245.051551	4201.452001	16.643085	-0.047856	3.533580
244.991636	4193.481439	16.648090	-0.047840	3.530397
244.974255	4185.432051	16.653095	-0.047831	3.527182
245.092763	4177.465524	16.658099	-0.047848	3.524000
244.848617	4169.548663	16.663104	-0.047797	3.520825
244.642588	4161.557448	16.668109	-0.047754	3.517618
244.902089	4153.540213	16.673114	-0.047797	3.514412
244.545419	4145.519279	16.678119	-0.047725	3.511182
244.540891	4137.525341	16.683123	-0.047719	3.507972
244.549291	4129.527637	16.688128	-0.047715	3.504757
244.423365	4121.554670	16.693133	-0.047686	3.501545
244.418193	4113.587443	16.698138	-0.047680	3.498336
244.425231	4105.582455	16.703143	-0.047676	3.495110
244.325889	4097.581573	16.708147	-0.047652	3.491879
244.300355	4089.578502	16.713152	-0.047642	3.488646
244.294043	4081.585218	16.718157	-0.047635	3.485414
244.653898	4073.609098	16.723162	-0.047697	3.482199
244.485733	4065.615580	16.728167	-0.047660	3.478956
244.215371	4057.673863	16.733171	-0.047605	3.475728
244.344248	4049.604166	16.738176	-0.047623	3.472458
244.341795	4041.578580	16.743181	-0.047618	3.469199
244.159915	4033.633951	16.748186	-0.047578	3.465964
244.028338	4025.636056	16.753191	-0.047549	3.462705
244.085525	4017.644435	16.758195	-0.047554	3.459452
244.062284	4009.675184	16.763200	-0.047544	3.456203
244.122124	4001.644048	16.768205	-0.047550	3.452928
244.068621	3993.630414	16.773210	-0.047535	3.449653
243.912677	3985.678500	16.778215	-0.047500	3.446397
243.842328	3977.679960	16.783219	-0.047482	3.443122
244.082607	3969.690505	16.788224	-0.047521	3.439858
244.001101	3961.721026	16.793229	-0.047501	3.436588
243.996258	3953.689802	16.798234	-0.047495	3.433292
243.871507	3945.673069	16.803239	-0.047466	3.429995
243.903686	3937.700572	16.808243	-0.047467	3.426718
243.822037	3929.697278	16.813248	-0.047446	3.423421
243.853328	3921.701522	16.818253	-0.047447	3.420129
243.892059	3913.750681	16.823258	-0.047449	3.416851
243.741449	3905.779276	16.828263	-0.047415	3.413556
243.379342	3897.762190	16.833267	-0.047342	3.410232
243.645170	3889.778603	16.838272	-0.047387	3.406939
243.489228	3881.788767	16.843277	-0.047352	3.403626
243.330654	3873.839392	16.848282	-0.047317	3.400327
243.194410	3865.872617	16.853287	-0.047287	3.397018
243.577258	3857.779162	16.858291	-0.047353	3.393671
243.398790	3849.727968	16.863296	-0.047314	3.390319
243.297203	3841.762361	16.868301	-0.047290	3.387002
243.420038	3833.802131	16.873306	-0.047307	3.383692
243.357770	3825.815155	16.878311	-0.047290	3.380361
243.134354	3817.858742	16.883315	-0.047244	3.377033
243.159227	3809.863002	16.888320	-0.047243	3.373695
243.188406	3801.819566	16.893325	-0.047243	3.370333
243.233779	3793.872246	16.898330	-0.047246	3.367009
243.104263	3785.862068	16.903335	-0.047217	3.363649
243.088441	3777.891130	16.908339	-0.047208	3.360307
243.029197	3769.945999	16.913344	-0.047192	3.356970
242.881707	3761.906486	16.918349	-0.047159	3.353587
243.125137	3753.892566	16.923354	-0.047199	3.350225
243.097629	3745.884849	16.928359	-0.047189	3.346853
242.878653	3737.909989	16.933363	-0.047143	3.343485
242.895490	3729.934591	16.938368	-0.047140	3.340121
242.906035	3721.945602	16.943373	-0.047137	3.336748
242.943000	3713.945402	16.948378	-0.047139	3.333368
242.774357	3705.938866	16.953383	-0.047102	3.329974
242.573379	3697.964044	16.958387	-0.047059	3.326589
242.780458	3689.991713	16.963392	-0.047092	3.323216
242.764611	3681.975720	16.968397	-0.047084	3.319814
242.624680	3674.074405	16.973402	-0.047053	3.316452
242.449511	3666.023607	16.978407	-0.047015	3.313021
242.555949	3657.957707	16.983411	-0.047029	3.309591
242.397596	3650.027649	16.988416	-0.046994	3.306206
242.329126	3642.031218	16.993421	-0.046976	3.302792
242.537960	3634.036587	16.998426	-0.047010	3.299386
242.422517	3626.084988	17.003431	-0.046983	3.295982
242.495274	3618.075921	17.008435	-0.046991	3.292558
242.294407	3610.091745	17.013440	-0.046949	3.289130
242.108803	3602.110981	17.018445	-0.046909	3.285700
242.174914	3594.136992	17.023450	-0.046916	3.282280
242.198783	3586.158410	17.028455	-0.046915	3.278852
242.027404	3578.155093	17.033459	-0.046878	3.275403
242.194039	3570.136097	17.038464	-0.046903	3.271956
242.031468	3562.116369	17.043469	-0.046868	3.268492
242.083064	3554.150032	17.048474	-0.046872	3.265057
241.928987	3546.188478	17.053479	-0.046838	3.261611
241.934172	3538.173919	17.058483	-0.046834	3.258145
242.049572	3530.204617	17.063488	-0.046850	3.254700
241.806117	3522.202568	17.068493	-0.046799	3.251222
241.689739	3514.226253	17.073498	-0.046772	3.247757
241.972742	3506.208665	17.078503	-0.046819	3.244287
241.799569	3498.261152	17.083507	-0.046782	3.240824
241.696748	3490.296333	17.088512	-0.046757	3.237353
241.891359	3482.225793	17.093517	-0.046788	3.233845
241.810882	3474.194565	17.098522	-0.046768	3.230339
241.687979	3466.226084	17.103527	-0.046740	3.226854
241.426903	3458.258504	17.108531	-0.046686	3.223361
241.639793	3450.287333	17.113536	-0.046720	3.219881
241.352049	3442.326850	17.118541	-0.046661	3.216382
241.272589	3434.334216	17.123546	-0.046641	3.212874
241.355984	3426.302296	17.128551	-0.046651	3.209351
241.445280	3418.298478	17.133555	-0.046663	3.205837
241.362588	3410.368623	17.138560	-0.046642	3.202344
241.353849	3402.372438	17.143565	-0.046635	3.198821
241.464187	3394.382232	17.148570	-0.046650	3.195303
241.135244	3386.396000	17.153575	-0.046584	3.191763
241.038247	3378.406523	17.158579	-0.046560	3.188228
241.151882	3370.387463	17.163584	-0.046576	3.184685
241.111350	3362.432918	17.168589	-0.046563	3.181160
241.313498	3354.432228	17.173594	-0.046595	3.177621
241.159926	3346.461251	17.178599	-0.046561	3.174076
240.926131	3338.461362	17.183603	-0.046513	3.170510
240.947184	3330.478916	17.188608	-0.046511	3.166960
240.867621	3322.485739	17.193613	-0.046491	3.163396
241.094580	3314.522243	17.198618	-0.046528	3.159855
240.989465	3306.553729	17.203623	-0.046503	3.156293
240.850436	3298.522170	17.208627	-0.046472	3.152697
241.024996	3290.499214	17.213632	-0.046499	3.149115
240.999051	3282.501437	17.218637	-0.046489	3.145531
240.762397	3274.577278	17.223642	-0.046439	3.141967
240.709517	3266.587889	17.228647	-0.046424	3.138378
240.742825	3258.584609	17.233651	-0.046425	3.134782
240.504430	3250.633932	17.238656	-0.046375	3.131194
240.472009	3242.607732	17.243661	-0.046364	3.127576
240.774400	3234.597126	17.248666	-0.046415	3.123976
240.598373	3226.656874	17.253671	-0.046377	3.120383
240.588358	3218.681066	17.258675	-0.046370	3.116777
240.693081	3210.685838	17.263680	-0.046384	3.113163
240.432247	3202.679162	17.268685	-0.046330	3.109523
240.167475	3194.734658	17.273690	-0.046275	3.105907
240.301520	3186.745177	17.278695	-0.046295	3.102284
240.348959	3178.739346	17.283699	-0.046299	3.098645
240.179680	3170.764684	17.288704	-0.046262	3.095007
240.178848	3162.747609	17.293709	-0.046256	3.091353
240.439982	3154.742981	17.298714	-0.046300	3.087712
240.408523	3146.763591	17.303719	-0.046288	3.084065
240.038713	3138.836802	17.308723	-0.046214	3.080422
240.042389	3130.878947	17.313728	-0.046210	3.076777
240.001067	3122.805805	17.318733	-0.046196	3.073074
239.823050	3114.790330	17.323738	-0.046158	3.069386
239.846337	3106.813588	17.328743	-0.046157	3.065720
239.872259	3098.847463	17.333747	-0.046157	3.062056
239.672763	3090.905835	17.338752	-0.046114	3.058387
239.593623	3082.896548	17.343757	-0.046094	3.054689
239.758263	3074.900982	17.348762	-0.046119	3.051004
239.694388	3066.946637	17.353767	-0.046102	3.047323
239.612451	3058.943149	17.358771	-0.046082	3.043614
239.959060	3050.963700	17.363776	-0.046141	3.039932
239.817461	3042.992565	17.368781	-0.046109	3.036226
239.705380	3035.008699	17.373786	-0.046083	3.032510
239.443458	3027.013376	17.378791	-0.046029	3.028778
239.571703	3018.989399	17.383795	-0.046047	3.025047
239.587345	3011.048562	17.388800	-0.046045	3.021344
239.503633	3003.042986	17.393805	-0.046024	3.017602
239.610453	2995.077474	17.398810	-0.046039	3.013883
239.633878	2987.061177	17.403815	-0.046038	3.010131
239.281279	2979.119703	17.408819	-0.045967	3.006392
239.407924	2971.141126	17.413824	-0.045985	3.002654
239.158429	2963.165641	17.418829	-0.045933	2.998894
239.261619	2955.196819	17.423834	-0.045947	2.995150
239.074714	2947.175910	17.428839	-0.045907	2.991362
239.162716	2939.152621	17.433843	-0.045918	2.987583
239.254736	2931.193851	17.438848	-0.045930	2.983829
238.963280	2923.215953	17.443853	-0.045870	2.980042
239.023660	2915.270117	17.448858	-0.045876	2.976283
238.974734	2907.266335	17.453863	-0.045862	2.972486
238.798965	2899.267328	17.458867	-0.045824	2.968680
238.843974	2891.319321	17.463872	-0.045827	2.964905
238.814174	2883.322579	17.468877	-0.045816	2.961098
238.779012	2875.345883	17.473882	-0.045804	2.957296
238.617264	2867.360424	17.478887	-0.045768	2.953478
238.735878	2859.326345	17.483891	-0.045785	2.949646
238.753756	2851.367688	17.488896	-0.045783	2.945840
238.499398	2843.404535	17.493901	-0.045730	2.942012
238.563381	2835.432258	17.498906	-0.045737	2.938192
238.665687	2827.431713	17.503911	-0.045751	2.934356
238.522990	2819.437143	17.508915	-0.045719	2.930504
238.655509	2811.449671	17.513920	-0.045738	2.926665
238.672852	2803.479387	17.518925	-0.045736	2.922824
238.598971	2795.532157	17.523930	-0.045717	2.918983
238.305836	2787.584645	17.528935	-0.045657	2.915126
238.459532	2779.452343	17.533939	-0.045680	2.911198
238.618277	2771.494526	17.538944	-0.045705	2.907349
238.096729	2763.551534	17.543949	-0.045602	2.903467
238.093677	2755.599996	17.548954	-0.045596	2.899602
238.109720	2747.634506	17.553959	-0.045594	2.895727
238.175571	2739.607556	17.558963	-0.045601	2.891819
238.180805	2731.631409	17.563968	-0.045597	2.887927
238.000239	2723.655408	17.568973	-0.045558	2.884020
238.216487	2715.690694	17.573978	-0.045593	2.880135
238.111464	2707.733659	17.578983	-0.045568	2.876231
237.960041	2699.732261	17.583987	-0.045534	2.872298
238.012854	2691.732983	17.588992	-0.045539	2.868371
237.764075	2683.747424	17.593997	-0.045487	2.864429
237.883904	2675.815126	17.599002	-0.045504	2.860528
237.931068	2667.827775	17.604007	-0.045508	2.856590
237.775469	2659.844615	17.609011	-0.045473	2.852638
237.661050	2651.884975	17.614016	-0.045447	2.848694
237.807665	2643.852059	17.619021	-0.045469	2.844724
237.926772	2635.923970	17.624026	-0.045485	2.840798
237.654631	2627.973987	17.629031	-0.045429	2.836833
237.583849	2619.949621	17.634035	-0.045411	2.832838
237.794828	2611.940812	17.639040	-0.045445	2.828860
237.751247	2603.944084	17.644045	-0.045431	2.824869
237.640987	2596.016275	17.649050	-0.045406	2.820902
237.591016	2588.049111	17.654055	-0.045391	2.816914
237.510685	2580.050657	17.659059	-0.045371	2.812903
237.453034	2572.084681	17.664064	-0.045355	2.808903
237.309354	2564.094037	17.669069	-0.045323	2.804880
237.275576	2556.148763	17.674074	-0.045311	2.800881
237.360848	2548.171993	17.679079	-0.045322	2.796867
237.273758	2540.165985	17.684083	-0.045300	2.792822
237.330322	2532.187687	17.689088	-0.045305	2.788794
237.035995	2524.206771	17.694093	-0.045245	2.784739
237.096610	2516.253601	17.699098	-0.045251	2.780712
237.265249	2508.253223	17.704103	-0.045277	2.776662
237.233691	2500.249735	17.709107	-0.045266	2.772592
237.239983	2492.300785	17.714112	-0.045262	2.768547
236.915862	2484.351347	17.719117	-0.045196	2.764475
236.951147	2476.397306	17.724122	-0.045197	2.760417
236.933004	2468.430707	17.729127	-0.045189	2.756343
236.773880	2460.369406	17.734131	-0.045154	2.752206
236.829921	2452.375866	17.739136	-0.045159	2.748111
236.756384	2444.397359	17.744141	-0.045140	2.744009
236.914225	2436.428327	17.749146	-0.045164	2.739920
236.720186	2428.499462	17.754151	-0.045122	2.735824
236.770161	2420.502217	17.759155	-0.045126	2.731702
236.769713	2412.525424	17.764160	-0.045121	2.727581
236.742521	2404.546986	17.769165	-0.045111	2.723451
236.627389	2396.618842	17.774170	-0.045084	2.719336
236.408834	2388.680853	17.779175	-0.045038	2.715203
236.494145	2380.617891	17.784179	-0.045048	2.711017
236.670196	2372.648146	17.789184	-0.045076	2.706879
236.546469	2364.690562	17.794189	-0.045048	2.702722
236.246976	2356.748492	17.799194	-0.044986	2.698556
236.358987	2348.766927	17.804199	-0.045002	2.694389
236.387684	2340.763619	17.809203	-0.045002	2.690199
236.294134	2332.807150	17.814208	-0.044979	2.686019
236.240981	2324.858231	17.819213	-0.044964	2.681839
236.301145	2316.884292	17.824218	-0.044970	2.677646
236.250090	2308.904934	17.829223	-0.044955	2.673437
236.009709	2300.900318	17.834227	-0.044905	2.669196
236.095336	2292.942029	17.839232	-0.044916	2.664993
235.858920	2284.987208	17.844237	-0.044866	2.660765
235.775277	2277.037094	17.849242	-0.044845	2.656543
235.873416	2269.021649	17.854247	-0.044858	2.652290
235.795601	2261.038211	17.859251	-0.044839	2.648037
235.945341	2253.063131	17.864256	-0.044861	2.643796
235.707625	2245.120619	17.869261	-0.044812	2.639540
235.849408	2237.158341	17.874266	-0.044833	2.635292
235.792973	2229.151711	17.879271	-0.044817	2.631000
235.699432	2221.185145	17.884275	-0.044794	2.626720
235.797128	2213.221608	17.889280	-0.044807	2.622448
235.538669	2205.262070	17.894285	-0.044753	2.618146
235.572458	2197.286449	17.899290	-0.044754	2.613849
235.557553	2189.300510	17.904295	-0.044746	2.609536
235.523732	2181.337342	17.909299	-0.044735	2.605226
235.487331	2173.407841	17.914304	-0.044723	2.600928
235.413060	2165.436987	17.919309	-0.044704	2.596597
235.339144	2157.335105	17.924314	-0.044684	2.592188
235.439190	2149.291432	17.929319	-0.044698	2.587815
235.029610	2141.386967	17.934323	-0.044616	2.583475
235.245317	2133.442039	17.939328	-0.044651	2.579149
235.256965	2125.474703	17.944333	-0.044648	2.574790
235.104376	2117.522195	17.949338	-0.044614	2.570419
235.034074	2109.577460	17.954343	-0.044596	2.566052
234.957743	2101.611609	17.959347	-0.044576	2.561664
234.773975	2093.704745	17.964352	-0.044537	2.557295
234.614523	2085.729584	17.969357	-0.044502	2.552882
234.758203	2077.719388	17.974362	-0.044523	2.548462
234.595977	2069.773150	17.979367	-0.044488	2.544050
234.446820	2061.820856	17.984371	-0.044455	2.539627
234.582046	2053.868124	17.989376	-0.044474	2.535216
234.563184	2045.860309	17.994381	-0.044466	2.530756
234.549037	2037.904881	17.999386	-0.044458	2.526317
234.649524	2029.952101	18.004391	-0.044471	2.521881
234.617942	2021.978089	18.009395	-0.044460	2.517415
234.679898	2014.016234	18.014400	-0.044466	2.512955
234.502875	2006.008712	18.019405	-0.044428	2.508444
234.575656	1998.037824	18.024410	-0.044436	2.503964
234.288376	1990.131772	18.029415	-0.044377	2.499486
234.064203	1982.181920	18.034419	-0.044330	2.494979
234.333489	1974.176072	18.039424	-0.044375	2.490469
234.427461	1966.176189	18.044429	-0.044387	2.485942
234.317399	1958.266742	18.049434	-0.044361	2.481442
234.213091	1950.322432	18.054439	-0.044337	2.476915
234.104600	1942.353024	18.059443	-0.044311	2.472365
234.173077	1934.369261	18.064448	-0.044319	2.467811
233.870503	1926.416474	18.069453	-0.044257	2.463239
234.131561	1918.433762	18.074458	-0.044300	2.458684
234.121231	1910.495518	18.079463	-0.044293	2.454125
233.826341	1902.525578	18.084467	-0.044233	2.449518
233.728324	1894.587973	18.089472	-0.044209	2.444936
233.688744	1886.630876	18.094477	-0.044196	2.440338
233.735993	1878.679239	18.099482	-0.044200	2.435742
233.660564	1870.657593	18.104487	-0.044181	2.431086
233.666266	1862.659968	18.109491	-0.044176	2.426442
233.703356	1854.706456	18.114496	-0.044178	2.421818
233.599145	1846.764360	18.119501	-0.044153	2.417180
233.699020	1838.792056	18.124506	-0.044166	2.412531
233.678717	1830.836628	18.129511	-0.044157	2.407874
233.473720	1822.894848	18.134515	-0.044114	2.403201
233.330502	1814.981903	18.139520	-0.044082	2.398542
233.274768	1807.007038	18.144525	-0.044066	2.393843
233.404093	1799.026293	18.149530	-0.044085	2.389146
233.390707	1791.063100	18.154535	-0.044077	2.384439
233.206385	1783.131172	18.159539	-0.044038	2.379728
233.323152	1775.171749	18.164544	-0.044054	2.375015
233.135071	1767.210003	18.169549	-0.044014	2.370267
232.954700	1759.279516	18.174554	-0.043975	2.365529
233.147133	1751.311106	18.179559	-0.044005	2.360788
232.909304	1743.378331	18.184563	-0.043956	2.356024
232.997124	1735.388309	18.189568	-0.043967	2.351243
233.031686	1727.408698	18.194573	-0.043968	2.346454
232.962159	1719.452463	18.199578	-0.043950	2.341661
232.989529	1711.510258	18.204583	-0.043949	2.336874
232.796063	1703.563741	18.209587	-0.043908	2.332057
233.117391	1695.569326	18.214592	-0.043963	2.327243
232.807851	1687.664406	18.219597	-0.043900	2.322422
232.645726	1679.738013	18.224602	-0.043864	2.317589
232.627919	1671.791877	18.229607	-0.043856	2.312746
232.393886	1663.814862	18.234611	-0.043807	2.307857
232.375085	1655.875593	18.239616	-0.043798	2.302997
232.124137	1647.944777	18.244621	-0.043746	2.298114
232.365631	1639.937625	18.249626	-0.043786	2.293214
232.295747	1631.993582	18.254631	-0.043767	2.288317
232.100065	1624.070031	18.259635	-0.043725	2.283411
232.441939	1616.088639	18.264640	-0.043784	2.278504
232.242319	1608.137684	18.269645	-0.043741	2.273560
232.068070	1600.142140	18.274650	-0.043704	2.268579
232.278109	1592.173599	18.279655	-0.043737	2.263637
232.198702	1584.247999	18.284659	-0.043717	2.258686
232.105184	1576.319833	18.289664	-0.043695	2.253721
231.955068	1568.360579	18.294669	-0.043661	2.248721
231.924972	1560.418522	18.299674	-0.043650	2.243730
231.818870	1552.515159	18.304679	-0.043625	2.238747
231.842583	1544.540110	18.309683	-0.043624	2.233719
231.975323	1536.567970	18.314688	-0.043644	2.228690
231.834959	1528.636995	18.319693	-0.043612	2.223652
231.757175	1520.704243	18.324698	-0.043593	2.218608
231.784763	1512.771085	18.329703	-0.043593	2.213560
231.638483	1504.808610	18.334707	-0.043560	2.208467
231.770553	1496.855831	18.339712	-0.043579	2.203394
231.507302	1488.952253	18.344717	-0.043525	2.198304
231.479564	1480.998909	18.349722	-0.043515	2.193192
231.533275	1473.019652	18.354727	-0.043519	2.188059
231.249051	1465.086432	18.359731	-0.043461	2.182913
231.439175	1457.145269	18.364736	-0.043491	2.177792
231.264603	1449.212192	18.369741	-0.043453	2.172632
231.197720	1441.267636	18.374746	-0.043436	2.167461
231.295429	1433.315262	18.379751	-0.043448	2.162289
231.184771	1425.392468	18.384755	-0.043423	2.157103
231.141203	1417.463245	18.389760	-0.043409	2.151908
230.999742	1409.516357	18.394765	-0.043377	2.146679
231.186983	1401.556751	18.399770	-0.043407	2.141459
230.914446	1393.671249	18.404775	-0.043351	2.136233
230.950541	1385.684249	18.409779	-0.043352	2.130956
230.791800	1377.775126	18.414784	-0.043318	2.125698
230.911130	1369.813232	18.419789	-0.043334	2.120419
230.640006	1361.932056	18.424794	-0.043279	2.115144
230.649692	1353.911567	18.429799	-0.043275	2.109789
230.746846	1345.938119	18.434803	-0.043288	2.104460
230.730502	1338.037910	18.439808	-0.043280	2.099156
230.700067	1330.110121	18.444813	-0.043269	2.093819
230.745602	1322.150613	18.449818	-0.043272	2.088454
230.636751	1314.254233	18.454823	-0.043246	2.083103
230.382362	1306.355708	18.459827	-0.043194	2.077722
230.419793	1298.421060	18.464832	-0.043195	2.072331
230.333860	1290.473782	18.469837	-0.043174	2.066905
230.356641	1282.525367	18.474842	-0.043173	2.061476
230.403708	1274.610908	18.479847	-0.043176	2.056057
230.273145	1266.663863	18.484851	-0.043147	2.050584
230.077653	1258.772308	18.489856	-0.043105	2.045128
230.044185	1250.850599	18.494861	-0.043094	2.039653
229.998984	1242.923754	18.499866	-0.043080	2.034159
229.949469	1234.968466	18.504871	-0.043065	2.028629
229.970712	1227.032953	18.509875	-0.043064	2.023105
230.048647	1219.105118	18.514880	-0.043073	2.017577
229.909615	1211.179133	18.519885	-0.043042	2.012013
229.717722	1203.258340	18.524890	-0.043001	2.006432
229.643648	1195.362394	18.529895	-0.042982	2.000865
229.762450	1187.420303	18.534899	-0.042999	1.995270
229.556338	1179.523786	18.539904	-0.042955	1.989657
229.327720	1171.613085	18.544909	-0.042907	1.984016
229.189204	1163.703949	18.549914	-0.042876	1.978369
229.400735	1155.750839	18.554919	-0.042910	1.972712
229.155208	1147.835523	18.559923	-0.042859	1.967017
229.085960	1139.934292	18.564928	-0.042841	1.961335
229.368916	1131.974883	18.569933	-0.042889	1.955632
229.002463	1124.061827	18.574938	-0.042815	1.949875
229.125012	1116.112097	18.579943	-0.042833	1.944128
229.322442	1108.156896	18.584947	-0.042864	1.938369
229.252498	1100.270960	18.589952	-0.042846	1.932613
229.036780	1092.364641	18.594957	-0.042800	1.926809
228.999667	1084.466387	18.599962	-0.042788	1.921013
228.962116	1076.573386	18.604967	-0.042776	1.915204
228.807583	1068.652318	18.609971	-0.042742	1.909342
228.625280	1060.768512	18.614976	-0.042703	1.903488
228.939285	1052.807966	18.619981	-0.042756	1.897614
228.717559	1044.922791	18.624986	-0.042709	1.891717
228.738883	1036.997640	18.629991	-0.042708	1.885800
228.542837	1029.118347	18.634995	-0.042666	1.879874
228.895172	1021.179803	18.640000	-0.042726	1.873947
228.652899	1013.277850	18.645005	-0.042676	1.867960
228.356904	1005.399108	18.650010	-0.042616	1.861966
228.712504	997.455891	18.655015	-0.042677	1.855979
228.509028	989.558532	18.660019	-0.042634	1.849942
228.481421	981.665007	18.665024	-0.042623	1.843909
228.360112	973.791563	18.670029	-0.042595	1.837861
228.055734	965.931322	18.675034	-0.042533	1.831781
228.062626	958.009075	18.680039	-0.042529	1.825670
228.057789	950.099615	18.685043	-0.042523	1.819547
228.110765	942.199390	18.690048	-0.042528	1.813417
227.795469	934.326322	18.695053	-0.042464	1.807243
227.947133	926.400363	18.700058	-0.042487	1.801063
227.968437	918.522221	18.705063	-0.042485	1.794884
227.740898	910.583491	18.710067	-0.042438	1.788605
227.689391	902.699691	18.715072	-0.042423	1.782369
227.802919	894.793648	18.720077	-0.042439	1.776114
227.780121	886.899719	18.725082	-0.042429	1.769829
227.664315	879.044401	18.730087	-0.042402	1.763541
227.534033	871.170814	18.735091	-0.042373	1.757215
227.586061	863.271983	18.740096	-0.042377	1.750868
227.318478	855.415613	18.745101	-0.042322	1.744491
227.197879	847.544953	18.750106	-0.042295	1.738099
227.401363	839.630448	18.755111	-0.042327	1.731688
227.419782	831.727109	18.760115	-0.042325	1.725239
227.232994	823.897116	18.765120	-0.042285	1.718800
227.212242	816.013812	18.770125	-0.042276	1.712314
227.054911	808.124686	18.775130	-0.042242	1.705780
227.103914	800.252125	18.780135	-0.042246	1.699262
227.153747	792.351852	18.785139	-0.042250	1.692697
226.892448	784.515300	18.790144	-0.042196	1.686117
226.920517	776.642897	18.795149	-0.042196	1.679520
226.869963	768.782525	18.800154	-0.042181	1.672897
226.933781	760.894744	18.805159	-0.042188	1.666240
226.600499	753.070266	18.810163	-0.042120	1.659556
226.606576	745.201457	18.815168	-0.042116	1.652853
226.676315	737.313743	18.820173	-0.042124	1.646116
226.850192	729.433413	18.825178	-0.042151	1.639371
226.558886	721.611153	18.830183	-0.042092	1.632585
226.272480	713.724646	18.835187	-0.042033	1.625715
226.407589	705.861721	18.840192	-0.042053	1.618895
226.286723	698.014784	18.845197	-0.042025	1.612024
226.138154	690.167446	18.850202	-0.041992	1.605120
226.150469	682.342789	18.855207	-0.041989	1.598228
226.096479	674.475669	18.860211	-0.041974	1.591260
225.931550	666.650517	18.865216	-0.041938	1.584283
225.976216	658.793172	18.870221	-0.041941	1.577276
226.053316	650.924558	18.875226	-0.041950	1.570232
225.896995	643.117568	18.880231	-0.041916	1.563178
225.963245	635.272373	18.885235	-0.041923	1.556090
225.905329	627.426671	18.890240	-0.041907	1.548951
225.645173	619.626553	18.895245	-0.041853	1.541791
225.573034	611.791778	18.900250	-0.041835	1.534593
225.753888	603.927797	18.905255	-0.041863	1.527372
225.651627	596.105915	18.910259	-0.041839	1.520113
225.483952	588.328065	18.915264	-0.041802	1.512851
225.500935	580.479431	18.920269	-0.041800	1.505515
225.688580	572.636594	18.925274	-0.041830	1.498176
225.434062	564.857491	18.930279	-0.041778	1.490792
225.318510	557.049262	18.935283	-0.041751	1.483365
225.220749	549.259138	18.940288	-0.041727	1.475920
225.241391	541.386893	18.945293	-0.041726	1.468378
225.140871	533.591351	18.950298	-0.041702	1.460852
225.120180	525.799241	18.955303	-0.041693	1.453302
225.022349	517.987948	18.960307	-0.041670	1.445683
224.880915	510.227900	18.965312	-0.041638	1.438065
224.818558	502.427152	18.970317	-0.041621	1.430381
224.802502	494.631841	18.975322	-0.041613	1.422667
224.762840	486.859137	18.980327	-0.041600	1.414930
224.363499	479.105927	18.985331	-0.041521	1.407110
224.514919	471.305851	18.990336	-0.041544	1.399292
224.449470	463.524083	18.995341	-0.041527	1.391411
224.324810	455.747070	19.000346	-0.041498	1.383480
224.456848	447.960733	19.005351	-0.041518	1.375538
224.348533	440.191908	19.010355	-0.041492	1.367527
224.308631	432.442778	19.015360	-0.041480	1.359500
224.180181	424.696997	19.020365	-0.041451	1.351414
224.038594	416.946904	19.025370	-0.041419	1.343272
223.956323	409.218348	19.030375	-0.041398	1.335114
223.656419	401.487128	19.035379	-0.041337	1.326864
223.892576	393.713678	19.040384	-0.041376	1.318613
223.866260	385.885607	19.045389	-0.041366	1.310204
223.636287	378.137200	19.050394	-0.041318	1.301791
223.458853	370.449180	19.055399	-0.041280	1.293397
223.758217	362.655968	19.060403	-0.041331	1.284922
223.560830	354.987692	19.065408	-0.041289	1.276436
223.454074	347.286022	19.070413	-0.041264	1.267872
223.190469	339.614317	19.075418	-0.041209	1.259255
223.219393	331.901950	19.080423	-0.041210	1.250588
223.202373	324.198734	19.085427	-0.041201	1.241862
223.050324	316.533367	19.090432	-0.041168	1.233091
223.035647	308.819234	19.095437	-0.041160	1.224228
222.796268	301.168566	19.100442	-0.041110	1.215330
222.992031	293.457674	19.105447	-0.041142	1.206382
222.969403	285.795732	19.110451	-0.041132	1.197381
222.798337	278.155915	19.115456	-0.041095	1.188308
222.746762	270.504810	19.120461	-0.041081	1.179176
222.681779	262.855582	19.125466	-0.041063	1.169973
222.673726	255.221306	19.130471	-0.041057	1.160726
222.401141	247.603941	19.135475	-0.041001	1.151371
222.489597	239.937710	19.140480	-0.041012	1.141954
222.458594	232.310871	19.145485	-0.041001	1.132483
222.131087	224.741388	19.150490	-0.040935	1.122940
221.986616	217.167912	19.155495	-0.040903	1.113350
221.866474	209.567153	19.160499	-0.040876	1.103647
221.792599	201.992399	19.165504	-0.040857	1.093902
221.752083	194.407636	19.170509	-0.040845	1.084064
221.833332	186.820385	19.175514	-0.040855	1.074159
221.819531	179.252539	19.180519	-0.040847	1.064167
221.382522	171.771013	19.185523	-0.040761	1.054097
221.503404	164.192895	19.190528	-0.040778	1.043930
221.589141	156.663380	19.195533	-0.040789	1.033721
221.249741	149.191018	19.200538	-0.040721	1.023388
221.204734	141.699277	19.205543	-0.040707	1.012993
221.106513	134.208939	19.210547	-0.040684	1.002479
220.890427	126.751771	19.215552	-0.040639	0.991872
220.746758	119.274811	19.220557	-0.040607	0.981139
220.661132	111.823680	19.225562	-0.040586	0.970340
220.529298	104.404761	19.230567	-0.040557	0.959455
220.287063	97.004906	19.235571	-0.040507	0.948445
220.280768	89.594239	19.240576	-0.040501	0.937351
220.178159	82.205040	19.245581	-0.040477	0.926131
219.324951	74.970158	19.250586	-0.040313	0.914809
218.709498	67.688971	19.255591	-0.040193	0.903337
218.126278	60.644760	19.260595	-0.040080	0.892101