Fri Mar 12 12:51:07 2021

Number of Points = 3624
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.888667	0.045121	0.000000	0.000052	0.718019

1.065273	0.013459	0.005005	0.000019	0.718018
0.940175	0.034469	0.010010	0.000042	0.718015
1.019207	0.023622	0.015014	0.000028	0.718021
1.017306	0.019410	0.020019	0.000028	0.718012
1.030230	0.020812	0.025024	0.000026	0.718019
0.940976	0.034726	0.030029	0.000043	0.718015
0.965335	0.029747	0.035034	0.000039	0.718013
1.027179	0.022594	0.040038	0.000027	0.718020
1.195759	-0.011114	0.045043	-0.000004	0.718013
1.164753	-0.000979	0.050048	0.000002	0.718021
1.149229	0.000554	0.055053	0.000005	0.718019
0.887151	0.045487	0.060058	0.000054	0.718015
1.188801	-0.004971	0.065062	-0.000002	0.718021
1.191278	-0.072563	0.070067	-0.000002	0.717888
1.244627	-0.172459	0.075072	-0.000012	0.717709
1.063505	-0.139693	0.080077	0.000022	0.717709
1.138232	-0.155499	0.085082	0.000009	0.717704
1.123250	-0.149838	0.090086	0.000012	0.717710
0.946113	-0.121888	0.095091	0.000045	0.717702
0.953989	-0.119944	0.100096	0.000044	0.717708
1.032691	-0.187030	0.105101	0.000029	0.717603
0.907882	-0.274928	0.110106	0.000053	0.717385
0.778262	-0.247507	0.115110	0.000077	0.717393
0.889184	-0.274100	0.120115	0.000056	0.717379
0.859470	-0.264396	0.125120	0.000062	0.717388
0.818293	-0.258766	0.130125	0.000070	0.717384
0.900832	-0.386207	0.135130	0.000055	0.717160
0.939491	-0.427462	0.140134	0.000048	0.717092
0.874350	-0.421271	0.145139	0.000060	0.717081
1.112630	-0.458595	0.150144	0.000016	0.717091
1.153404	-0.524007	0.155149	0.000009	0.716975
1.043521	-0.614506	0.160154	0.000030	0.716757
0.998799	-0.603788	0.165158	0.000038	0.716762
0.820810	-0.575324	0.170163	0.000071	0.716755
1.141291	-0.711151	0.175168	0.000012	0.716599
0.876090	-0.734829	0.180173	0.000062	0.716458
0.702165	-0.708387	0.185178	0.000094	0.716449
0.796839	-0.719624	0.190182	0.000077	0.716460
0.650625	-0.857624	0.195187	0.000104	0.716134
0.847711	-0.890967	0.200192	0.000068	0.716138
1.037298	-0.922778	0.205197	0.000033	0.716141
0.802928	-0.979865	0.210202	0.000077	0.715945
0.962988	-1.032646	0.215206	0.000047	0.715896
0.841616	-1.016231	0.220211	0.000070	0.715886
0.839259	-1.147367	0.225216	0.000071	0.715625
0.797475	-1.175281	0.230221	0.000079	0.715554
0.770853	-1.172081	0.235226	0.000084	0.715551
0.850603	-1.339266	0.240230	0.000069	0.715247
0.759629	-1.328851	0.245235	0.000086	0.715235
0.690086	-1.371116	0.250240	0.000099	0.715126
0.925040	-1.520046	0.255245	0.000056	0.714913
0.753002	-1.491018	0.260250	0.000088	0.714910
0.643032	-1.592345	0.265254	0.000109	0.714669
0.768936	-1.644857	0.270259	0.000086	0.714609
0.735911	-1.707021	0.275264	0.000092	0.714474
0.627200	-1.782448	0.280269	0.000113	0.714285
0.669648	-1.807935	0.285274	0.000105	0.714249
0.742504	-1.957904	0.290278	0.000092	0.713977
0.370257	-1.893947	0.295283	0.000161	0.713971
0.186687	-1.991894	0.300288	0.000196	0.713711
0.417633	-2.060294	0.305293	0.000153	0.713657
0.307872	-2.128712	0.310298	0.000173	0.713482
0.220910	-2.170798	0.315302	0.000190	0.713367
0.211519	-2.237445	0.320307	0.000192	0.713230
-0.293217	-2.250889	0.325312	0.000286	0.713024
-1.279979	-2.075316	0.330317	0.000470	0.713023
-1.852351	-2.132230	0.335322	0.000577	0.712707
-1.868675	-2.123996	0.340326	0.000580	0.712717
-2.188990	-2.104093	0.345331	0.000640	0.712643
-2.716794	-2.135041	0.350336	0.000738	0.712393
-2.724432	-2.134667	0.355341	0.000740	0.712391
-3.088106	-2.092248	0.360346	0.000808	0.712346
-3.100694	-2.213729	0.365350	0.000810	0.712099
-3.762045	-2.100592	0.370355	0.000934	0.712089
-4.035072	-2.049756	0.375360	0.000985	0.712093
-3.448469	-2.286143	0.380365	0.000876	0.711830
-4.731445	-2.092342	0.385370	0.001115	0.711760
-4.753637	-2.085106	0.390374	0.001119	0.711767
-4.122288	-2.232454	0.395379	0.001002	0.711697
-5.483902	-2.109322	0.400384	0.001255	0.711458
-5.434732	-2.116565	0.405389	0.001246	0.711461
-5.650818	-2.082214	0.410394	0.001287	0.711452
-5.365167	-2.135900	0.415398	0.001234	0.711446
-6.199652	-2.141620	0.420403	0.001390	0.711138
-6.569963	-2.074034	0.425408	0.001459	0.711141
-6.444016	-2.094137	0.430413	0.001435	0.711145
-6.297760	-2.124352	0.435418	0.001408	0.711136
-6.407928	-2.144659	0.440422	0.001429	0.711056
-7.421858	-2.055054	0.445427	0.001618	0.710874
-7.043219	-2.120032	0.450432	0.001548	0.710879
-7.525432	-2.034616	0.455437	0.001638	0.710877
-7.615643	-2.020580	0.460442	0.001655	0.710873
-6.935505	-2.187060	0.465446	0.001528	0.710782
-8.198387	-2.087480	0.470451	0.001764	0.710531
-8.170247	-2.089414	0.475456	0.001759	0.710537
-8.023698	-2.113230	0.480461	0.001731	0.710541
-8.240169	-2.080210	0.485466	0.001772	0.710529
-8.408017	-2.045029	0.490470	0.001803	0.710540
-8.361485	-2.165113	0.495475	0.001795	0.710316
-8.823713	-2.130130	0.500480	0.001881	0.710221
-8.746763	-2.142013	0.505485	0.001867	0.710224
-9.482986	-2.014528	0.510490	0.002004	0.710216
-9.083229	-2.079955	0.515494	0.001930	0.710228
-9.033104	-2.092331	0.520499	0.001921	0.710220
-9.873650	-2.102144	0.525504	0.002078	0.709901
-9.664599	-2.139835	0.530509	0.002039	0.709900
-10.128277	-2.061111	0.535514	0.002126	0.709891
-10.053496	-2.070033	0.540518	0.002112	0.709900
-10.042771	-2.075620	0.545523	0.002110	0.709892
-9.950620	-2.089941	0.550528	0.002093	0.709896
-10.046736	-2.173140	0.555533	0.002111	0.709695
-11.200500	-2.015919	0.560538	0.002326	0.709598
-10.414892	-2.152110	0.565542	0.002180	0.709605
-10.713632	-2.102465	0.570547	0.002236	0.709598
-11.330357	-1.991234	0.575552	0.002351	0.709600
-10.501970	-2.135750	0.580557	0.002197	0.709606
-10.620086	-2.182330	0.585562	0.002219	0.709470
-12.233681	-1.993147	0.590566	0.002520	0.709273
-12.000295	-2.037555	0.595571	0.002476	0.709267
-11.789065	-2.073998	0.600576	0.002437	0.709269
-11.670926	-2.092016	0.605581	0.002416	0.709275
-12.062577	-2.026707	0.610586	0.002489	0.709265
-11.932454	-2.046159	0.615590	0.002465	0.709272
-11.698929	-2.133886	0.620595	0.002421	0.709180
-12.856724	-2.035831	0.625600	0.002637	0.708962
-12.234713	-2.143537	0.630605	0.002522	0.708968
-12.685973	-2.068692	0.635610	0.002606	0.708957
-12.703776	-2.062562	0.640614	0.002609	0.708962
-12.789173	-2.050272	0.645619	0.002625	0.708956
-12.542034	-2.090620	0.650624	0.002580	0.708963
-12.587615	-2.181634	0.655629	0.002588	0.708764
-14.048642	-1.982859	0.660634	0.002860	0.708641
-13.292470	-2.112726	0.665638	0.002720	0.708650
-13.286822	-2.118025	0.670643	0.002719	0.708641
-13.811984	-2.021587	0.675648	0.002817	0.708646
-13.764891	-2.028505	0.680653	0.002808	0.708649
-13.584205	-2.065040	0.685658	0.002775	0.708640
-13.803436	-2.114537	0.690662	0.002816	0.708462
-14.929072	-1.967950	0.695667	0.003026	0.708353
-14.370545	-2.066724	0.700672	0.002922	0.708355
-13.986690	-2.133159	0.705677	0.002851	0.708358
-14.800429	-1.992141	0.710682	0.003002	0.708350
-14.618575	-2.018561	0.715686	0.002969	0.708361
-14.253774	-2.085728	0.720691	0.002901	0.708357
-14.600022	-2.115392	0.725696	0.002966	0.708173
-15.682869	-1.997116	0.730701	0.003167	0.708023
-15.411930	-2.049423	0.735706	0.003117	0.708015
-15.357840	-2.054865	0.740710	0.003107	0.708023
-15.585252	-2.017413	0.745715	0.003150	0.708016
-15.129038	-2.096669	0.750720	0.003065	0.708020
-14.947028	-2.128609	0.755725	0.003031	0.708020
-15.773067	-2.064223	0.760730	0.003185	0.707854
-16.508931	-2.005653	0.765734	0.003323	0.707708
-15.933885	-2.110179	0.770739	0.003216	0.707704
-16.409389	-2.023757	0.775744	0.003305	0.707706
-16.452001	-2.013443	0.780749	0.003313	0.707712
-16.275808	-2.048783	0.785754	0.003280	0.707703
-16.174194	-2.062892	0.790758	0.003261	0.707711
-16.644925	-2.000358	0.795763	0.003349	0.707668
-17.270624	-2.030177	0.800768	0.003466	0.707384
-16.839332	-2.104607	0.805773	0.003386	0.707388
-17.544927	-1.984212	0.810778	0.003517	0.707377
-17.304445	-2.023814	0.815782	0.003473	0.707383
-16.966718	-2.086663	0.820787	0.003410	0.707378
-17.227337	-2.040486	0.825792	0.003459	0.707377
-17.138160	-2.052925	0.830797	0.003442	0.707383
-17.832746	-2.073631	0.835802	0.003572	0.707093
-18.041229	-2.038224	0.840806	0.003611	0.707089
-18.164865	-2.018563	0.845811	0.003634	0.707084
-18.084214	-2.033489	0.850816	0.003619	0.707082
-17.741743	-2.091351	0.855821	0.003556	0.707088
-18.134447	-2.025439	0.860826	0.003629	0.707080
-18.036916	-2.037231	0.865830	0.003611	0.707091
-18.415584	-2.128486	0.870835	0.003682	0.706771
-18.947410	-2.040725	0.875840	0.003781	0.706757
-18.991933	-2.030618	0.880845	0.003790	0.706761
-18.919483	-2.049017	0.885850	0.003776	0.706749
-18.742078	-2.075904	0.890854	0.003743	0.706759
-19.138822	-2.007870	0.895859	0.003817	0.706753
-18.896225	-2.051002	0.900864	0.003773	0.706753
-19.109573	-2.160730	0.905869	0.003813	0.706455
-19.843391	-2.037424	0.910874	0.003949	0.706440
-19.950067	-2.014064	0.915878	0.003969	0.706448
-19.538356	-2.088236	0.920883	0.003893	0.706446
-19.672024	-2.064608	0.925888	0.003918	0.706446
-19.958064	-2.011177	0.930893	0.003971	0.706450
-19.948199	-2.032128	0.935898	0.003970	0.706411
-20.399911	-2.088147	0.940902	0.004054	0.706136
-20.509508	-2.070595	0.945907	0.004075	0.706132
-20.740143	-2.029914	0.950912	0.004118	0.706131
-20.099321	-2.141435	0.955917	0.003999	0.706136
-20.853200	-2.011557	0.960922	0.004139	0.706126
-20.790954	-2.017028	0.965926	0.004128	0.706137
-20.496848	-2.107817	0.970931	0.004073	0.706060
-21.467243	-2.031369	0.975936	0.004254	0.705865
-21.125690	-2.089971	0.980941	0.004191	0.705869
-21.654761	-1.998456	0.985946	0.004289	0.705863
-21.312664	-2.054322	0.990950	0.004226	0.705873
-21.485210	-2.027022	0.995955	0.004258	0.705866
-21.722596	-1.984205	1.000960	0.004303	0.705867
-21.215190	-2.152349	1.005965	0.004209	0.705710
-22.464862	-2.021872	1.010970	0.004441	0.705524
-22.238606	-2.057750	1.015974	0.004399	0.705533
-22.154535	-2.075652	1.020979	0.004384	0.705526
-22.414663	-2.029323	1.025984	0.004433	0.705526
-22.076133	-2.085836	1.030989	0.004370	0.705533
-22.679884	-1.983759	1.035994	0.004482	0.705522
-22.488717	-2.119610	1.040998	0.004447	0.705316
-23.229801	-2.039459	1.046003	0.004585	0.705211
-23.356349	-2.017059	1.051008	0.004609	0.705211
-23.206548	-2.040899	1.056013	0.004581	0.705216
-23.523802	-1.988030	1.061018	0.004640	0.705208
-23.528124	-1.982534	1.066022	0.004641	0.705217
-23.207285	-2.042643	1.071027	0.004582	0.705211
-23.362259	-2.088213	1.076032	0.004611	0.705063
-24.332754	-2.000199	1.081037	0.004792	0.704892
-24.203740	-2.025412	1.086042	0.004768	0.704887
-23.984779	-2.061507	1.091046	0.004728	0.704893
-24.156080	-2.033569	1.096051	0.004760	0.704887
-24.345422	-1.998772	1.101056	0.004795	0.704889
-24.023654	-2.053040	1.106061	0.004735	0.704895
-24.086619	-2.096728	1.111066	0.004747	0.704784
-25.000351	-2.026853	1.116070	0.004918	0.704596
-24.888232	-2.049092	1.121075	0.004897	0.704591
-25.051467	-2.020266	1.126080	0.004927	0.704590
-24.652322	-2.086782	1.131085	0.004853	0.704599
-24.857130	-2.055077	1.136090	0.004892	0.704589
-24.643813	-2.088928	1.141094	0.004852	0.704597
-24.943215	-2.162586	1.146099	0.004908	0.704340
-26.112932	-1.993775	1.151104	0.005126	0.704260
-25.586673	-2.084622	1.156109	0.005028	0.704266
-25.699875	-2.068974	1.161114	0.005050	0.704256
-26.034667	-2.005264	1.166118	0.005112	0.704264
-25.901169	-2.028875	1.171123	0.005087	0.704264
-25.701318	-2.066368	1.176128	0.005051	0.704260
-26.182098	-2.114783	1.181133	0.005140	0.703989
-27.254656	-1.942063	1.186138	0.005340	0.703951
-26.804399	-2.017621	1.191142	0.005256	0.703960
-26.330843	-2.103060	1.196147	0.005169	0.703958
-27.308712	-1.928375	1.201152	0.005351	0.703958
-26.878851	-2.002851	1.206157	0.005271	0.703962
-26.662248	-2.045304	1.211162	0.005231	0.703954
-26.866858	-2.101229	1.216166	0.005269	0.703767
-28.092820	-1.946330	1.221171	0.005498	0.703638
-27.455712	-2.062594	1.226176	0.005379	0.703633
-27.267820	-2.091766	1.231181	0.005344	0.703641
-27.929214	-1.977524	1.236186	0.005468	0.703633
-27.621686	-2.028645	1.241190	0.005411	0.703640
-27.509143	-2.049488	1.246195	0.005390	0.703638
-27.860559	-2.068598	1.251200	0.005456	0.703473
-28.512674	-2.011767	1.256205	0.005577	0.703353
-28.241180	-2.066402	1.261210	0.005527	0.703340
-28.529353	-2.010850	1.266214	0.005581	0.703348
-28.580050	-2.003323	1.271219	0.005590	0.703344
-28.272262	-2.059326	1.276224	0.005533	0.703342
-28.191341	-2.068963	1.281229	0.005518	0.703351
-28.949078	-2.068120	1.286234	0.005660	0.703079
-29.413883	-2.016438	1.291238	0.005746	0.703016
-29.083929	-2.077127	1.296243	0.005685	0.703012
-29.371460	-2.027333	1.301248	0.005739	0.703009
-29.437155	-2.010562	1.306253	0.005751	0.703018
-29.398431	-2.021489	1.311258	0.005744	0.703010
-29.158633	-2.061389	1.316262	0.005700	0.703015
-29.990484	-2.044054	1.321267	0.005855	0.702750
-30.607434	-1.959124	1.326272	0.005970	0.702699
-29.996933	-2.064119	1.331277	0.005856	0.702707
-30.139297	-2.044031	1.336282	0.005883	0.702696
-30.384389	-1.997167	1.341286	0.005929	0.702702
-30.269794	-2.017603	1.346291	0.005908	0.702701
-30.210671	-2.030737	1.351296	0.005897	0.702696
-30.523107	-2.075292	1.356301	0.005955	0.702493
-31.336605	-1.989937	1.361306	0.006107	0.702372
-31.018461	-2.042692	1.366310	0.006048	0.702379
-30.847273	-2.074995	1.371315	0.006016	0.702375
-31.153403	-2.022692	1.376320	0.006074	0.702370
-30.824401	-2.076031	1.381325	0.006013	0.702381
-31.247623	-2.006479	1.386330	0.006091	0.702368
-31.578643	-2.060637	1.391334	0.006153	0.702139
-31.824236	-2.046450	1.396339	0.006199	0.702079
-32.115678	-1.997381	1.401344	0.006254	0.702073
-31.828461	-2.044546	1.406349	0.006200	0.702080
-31.896581	-2.037652	1.411354	0.006213	0.702069
-31.838520	-2.044651	1.416358	0.006203	0.702076
-31.768933	-2.055442	1.421363	0.006190	0.702079
-32.716766	-2.047822	1.426368	0.006367	0.701752
-32.651651	-2.058781	1.431373	0.006355	0.701753
-33.057858	-1.991714	1.436378	0.006431	0.701741
-32.797317	-2.035399	1.441382	0.006382	0.701747
-32.703456	-2.052679	1.446387	0.006365	0.701745
-32.798323	-2.036769	1.451392	0.006383	0.701743
-32.679108	-2.063084	1.456397	0.006361	0.701732
-33.509035	-2.062946	1.461402	0.006516	0.701433
-33.393642	-2.078476	1.466406	0.006494	0.701442
-33.609718	-2.040528	1.471411	0.006535	0.701441
-33.670893	-2.031550	1.476416	0.006546	0.701436
-33.336048	-2.087947	1.481421	0.006484	0.701443
-33.603337	-2.045570	1.486426	0.006534	0.701432
-33.779969	-2.074909	1.491430	0.006567	0.701308
-34.418734	-2.051387	1.496435	0.006686	0.701125
-34.346714	-2.066314	1.501440	0.006673	0.701120
-34.529442	-2.028724	1.506445	0.006707	0.701130
-34.943607	-1.958880	1.511450	0.006785	0.701121
-34.527197	-2.029979	1.516454	0.006707	0.701127
-34.478205	-2.037717	1.521459	0.006698	0.701129
-34.632673	-2.048401	1.526464	0.006727	0.701051
-34.729972	-2.112346	1.531469	0.006746	0.700886
-35.081719	-2.055749	1.536474	0.006811	0.700873
-35.511376	-1.975975	1.541478	0.006892	0.700879
-34.891433	-2.085991	1.546483	0.006776	0.700880
-34.945213	-2.079871	1.551488	0.006787	0.700873
-35.044354	-2.092972	1.556493	0.006805	0.700810
-36.035844	-2.051606	1.561498	0.006990	0.700535
-35.666656	-2.115406	1.566502	0.006921	0.700539
-36.226005	-2.013774	1.571507	0.007026	0.700542
-36.122340	-2.035845	1.576512	0.007007	0.700535
-35.815580	-2.085662	1.581517	0.006950	0.700544
-36.159117	-2.029986	1.586522	0.007014	0.700532
-36.475630	-2.071672	1.591526	0.007073	0.700333
-36.985752	-2.035587	1.596531	0.007168	0.700221
-36.880867	-2.056257	1.601536	0.007149	0.700217
-37.067756	-2.017891	1.606541	0.007184	0.700227
-37.263355	-1.987284	1.611546	0.007220	0.700218
-37.004392	-2.030082	1.616550	0.007172	0.700224
-36.810522	-2.064274	1.621555	0.007137	0.700225
-37.501843	-2.030878	1.626560	0.007266	0.700042
-37.849358	-2.036267	1.631565	0.007330	0.699905
-37.737194	-2.061274	1.636570	0.007310	0.699894
-38.127456	-1.990640	1.641574	0.007383	0.699896
-37.834587	-2.040411	1.646579	0.007328	0.699901
-37.919097	-2.030805	1.651584	0.007344	0.699889
-37.881821	-2.031532	1.656589	0.007337	0.699901
-38.073851	-2.066289	1.661594	0.007373	0.699760
-38.857448	-2.004797	1.666598	0.007519	0.699601
-38.406677	-2.084268	1.671603	0.007436	0.699603
-38.950162	-1.990422	1.676608	0.007537	0.699596
-38.680284	-2.034056	1.681613	0.007487	0.699605
-38.760984	-2.024127	1.686618	0.007502	0.699595
-38.972047	-1.984106	1.691622	0.007542	0.699600
-38.648873	-2.127588	1.696627	0.007482	0.699425
-39.818651	-1.997450	1.701632	0.007700	0.699265
-39.824495	-1.993106	1.706637	0.007701	0.699272
-39.970424	-1.969543	1.711642	0.007728	0.699266
-39.740106	-2.009353	1.716646	0.007686	0.699268
-39.374466	-2.073836	1.721651	0.007618	0.699269
-39.952134	-1.974235	1.726656	0.007726	0.699262
-39.755915	-2.065949	1.731661	0.007689	0.699147
-40.196019	-2.081428	1.736666	0.007772	0.698955
-40.564680	-2.014644	1.741670	0.007840	0.698957
-40.613422	-2.003226	1.746675	0.007850	0.698962
-40.628063	-2.004382	1.751680	0.007853	0.698954
-40.260149	-2.067236	1.756685	0.007784	0.698959
-40.715361	-1.988012	1.761690	0.007869	0.698955
-40.825866	-2.040088	1.766694	0.007890	0.698809
-41.201149	-2.053641	1.771699	0.007960	0.698645
-41.410880	-2.020039	1.776704	0.007999	0.698637
-41.286659	-2.037091	1.781709	0.007976	0.698647
-41.312879	-2.036525	1.786714	0.007981	0.698638
-41.614316	-1.980846	1.791718	0.008038	0.698641
-40.998974	-2.089867	1.796723	0.007923	0.698642
-41.241839	-2.149702	1.801728	0.007969	0.698432
-42.290199	-1.997840	1.806733	0.008164	0.698361
-42.555199	-1.955568	1.811738	0.008214	0.698350
-41.835166	-2.082112	1.816742	0.008080	0.698353
-41.633125	-2.115655	1.821747	0.008043	0.698358
-42.544198	-1.958574	1.826752	0.008212	0.698347
-42.277038	-2.011791	1.831757	0.008163	0.698335
-42.593951	-2.113262	1.836762	0.008222	0.698013
-42.777495	-2.078111	1.841766	0.008256	0.698018
-43.202376	-2.000376	1.846771	0.008336	0.698021
-43.283247	-1.988371	1.851776	0.008351	0.698016
-42.980488	-2.039957	1.856781	0.008295	0.698021
-43.199367	-2.003107	1.861786	0.008336	0.698016
-43.074214	-2.052625	1.866790	0.008313	0.697960
-43.714514	-2.062130	1.871795	0.008432	0.697708
-44.086994	-1.998801	1.876800	0.008502	0.697701
-43.942727	-2.019167	1.881805	0.008475	0.697712
-43.822635	-2.045229	1.886810	0.008453	0.697702
-44.177803	-1.982151	1.891814	0.008519	0.697701
-44.350740	-1.947972	1.896819	0.008551	0.697707
-44.159094	-1.986949	1.901824	0.008516	0.697697
-44.231690	-2.113949	1.906829	0.008530	0.697412
-45.164042	-1.962672	1.911834	0.008703	0.697381
-45.062751	-1.979937	1.916838	0.008685	0.697382
-44.273236	-2.119000	1.921843	0.008538	0.697385
-44.864373	-2.018698	1.926848	0.008648	0.697374
-44.973035	-1.992995	1.931853	0.008669	0.697387
-44.596326	-2.081880	1.936858	0.008599	0.697342
-45.431278	-2.059800	1.941862	0.008754	0.697083
-45.631345	-2.021588	1.946867	0.008792	0.697088
-45.885510	-1.979855	1.951872	0.008839	0.697081
-45.260857	-2.086336	1.956877	0.008723	0.697090
-45.509920	-2.046318	1.961882	0.008770	0.697081
-45.571828	-2.034703	1.966886	0.008782	0.697082
-45.246265	-2.179600	1.971891	0.008721	0.696904
-46.516629	-2.028010	1.976896	0.008958	0.696751
-46.542330	-2.018451	1.981901	0.008963	0.696761
-46.136167	-2.094425	1.986906	0.008887	0.696753
-46.706210	-1.991290	1.991910	0.008994	0.696756
-46.437831	-2.037327	1.996915	0.008944	0.696759
-46.449697	-2.096641	2.001920	0.008946	0.696633

-47.452720	-2.007746	2.011917	0.009134	0.696449
-47.115170	-2.068768	2.021914	0.009071	0.696447
-47.278042	-2.037000	2.031910	0.009102	0.696451
-47.278610	-2.037440	2.041907	0.009102	0.696450
-47.163986	-2.058658	2.051904	0.009081	0.696447
-47.465766	-2.005176	2.061901	0.009138	0.696446
-47.342557	-2.024860	2.071898	0.009115	0.696450
-47.275361	-2.034936	2.081894	0.009103	0.696453
-47.422140	-2.008682	2.091891	0.009131	0.696452
-47.206703	-2.047960	2.101888	0.009091	0.696450
-47.290653	-2.024790	2.111885	0.009107	0.696466
-46.530633	-2.018063	2.121882	0.008966	0.696755
-46.489816	-2.023318	2.131878	0.008959	0.696758
-46.151041	-2.083791	2.141875	0.008896	0.696757
-46.522953	-2.018836	2.151872	0.008966	0.696754
-46.577499	-2.008076	2.161869	0.008977	0.696755
-46.161610	-2.044045	2.171866	0.008900	0.696832
-45.507212	-2.035732	2.181862	0.008778	0.697086
-45.430190	-2.047866	2.191859	0.008764	0.697089
-45.606887	-2.017849	2.201856	0.008797	0.697085
-45.466499	-2.042436	2.211853	0.008772	0.697085
-44.789913	-2.051383	2.221850	0.008646	0.697312
-44.744250	-2.024849	2.231846	0.008638	0.697382
-44.406133	-2.084818	2.241843	0.008575	0.697382
-44.685827	-2.036624	2.251840	0.008628	0.697378
-44.211634	-2.013604	2.261837	0.008540	0.697596
-43.701641	-2.050720	2.271834	0.008445	0.697705
-43.772125	-2.037540	2.281830	0.008459	0.697705
-43.639454	-2.064165	2.291827	0.008435	0.697699
-43.171261	-2.016903	2.301824	0.008348	0.697964
-42.954816	-2.029630	2.311821	0.008308	0.698016
-42.673239	-2.079051	2.321818	0.008256	0.698017
-43.070301	-1.974630	2.331814	0.008330	0.698084
-42.019567	-2.027772	2.341811	0.008135	0.698357
-42.119339	-2.010598	2.351808	0.008154	0.698355
-41.997523	-2.033407	2.361805	0.008132	0.698352
-41.642670	-1.995897	2.371802	0.008066	0.698556
-41.171207	-2.036015	2.381798	0.007979	0.698644
-41.265503	-2.021010	2.391795	0.007997	0.698640
-41.302919	-1.971170	2.401792	0.008004	0.698727
-40.269540	-2.041964	2.411789	0.007812	0.698957
-40.401369	-2.017036	2.421786	0.007837	0.698959
-40.287769	-2.036304	2.431782	0.007816	0.698960
-39.593014	-2.042584	2.441779	0.007687	0.699199
-39.764857	-1.979161	2.451776	0.007719	0.699264
-39.537148	-2.018932	2.461773	0.007677	0.699265
-39.434980	-1.974243	2.471770	0.007659	0.699392
-38.582880	-2.023558	2.481766	0.007501	0.699600
-38.593369	-2.022234	2.491763	0.007503	0.699598
-38.798812	-1.984062	2.501760	0.007542	0.699600
-37.777041	-2.026669	2.511757	0.007352	0.699883
-37.958834	-1.987169	2.521754	0.007386	0.699897
-37.700379	-2.031420	2.531750	0.007338	0.699900
-37.485459	-1.986861	2.541747	0.007299	0.700067
-37.073644	-1.984678	2.551744	0.007222	0.700220
-36.875425	-2.019456	2.561741	0.007186	0.700220
-36.781001	-2.032796	2.571738	0.007169	0.700226
-36.080630	-2.002297	2.581734	0.007039	0.700541
-35.831697	-2.046620	2.591731	0.006993	0.700540
-36.002708	-2.016787	2.601728	0.007025	0.700538
-35.690619	-2.016853	2.611725	0.006967	0.700650
-35.072400	-2.016155	2.621722	0.006852	0.700874
-34.855090	-2.053064	2.631718	0.006812	0.700877
-34.958336	-2.032654	2.641715	0.006832	0.700880
-34.632292	-2.010257	2.651712	0.006772	0.701042
-34.447968	-2.002082	2.661709	0.006738	0.701125
-34.479392	-1.994866	2.671706	0.006744	0.701127
-34.087411	-1.991954	2.681702	0.006671	0.701274
-33.521294	-2.010387	2.691699	0.006566	0.701440
-33.705291	-1.978396	2.701696	0.006601	0.701438
-33.474421	-1.980813	2.711693	0.006558	0.701516
-32.556918	-2.030282	2.721690	0.006388	0.701746
-32.456762	-2.045639	2.731686	0.006370	0.701750
-32.930034	-1.961797	2.741683	0.006458	0.701748
-31.827058	-2.015165	2.751680	0.006253	0.702037
-31.792364	-2.003354	2.761677	0.006247	0.702073
-31.828960	-1.995601	2.771674	0.006254	0.702075
-31.497503	-1.992766	2.781670	0.006193	0.702199
-30.934191	-2.006134	2.791667	0.006089	0.702375
-30.919261	-2.007761	2.801664	0.006086	0.702376
-30.862991	-2.018576	2.811661	0.006076	0.702374
-30.031112	-2.012673	2.821658	0.005922	0.702684
-29.692720	-2.065012	2.831654	0.005859	0.702700
-30.153617	-1.983345	2.841651	0.005945	0.702698
-29.693406	-2.020002	2.851648	0.005860	0.702789
-29.165805	-2.004519	2.861645	0.005762	0.703010
-28.899772	-2.049950	2.871642	0.005713	0.703013
-29.094978	-2.015463	2.881638	0.005750	0.703011
-28.415987	-2.006226	2.891635	0.005624	0.703274
-28.190015	-2.009711	2.901632	0.005582	0.703347
-28.137562	-2.018337	2.911629	0.005573	0.703348
-28.107521	-1.991685	2.921626	0.005567	0.703412
-27.255830	-2.028845	2.931622	0.005409	0.703643
-27.348037	-2.011988	2.941619	0.005427	0.703643
-27.141342	-2.050515	2.951616	0.005389	0.703639
-27.126380	-1.941321	2.961613	0.005386	0.703863
-26.431677	-2.019158	2.971610	0.005257	0.703955
-26.464880	-2.011117	2.981606	0.005264	0.703959
-26.321822	-1.979822	2.991603	0.005238	0.704073
-25.684937	-1.999423	3.001600	0.005119	0.704261
-25.781066	-1.980395	3.011597	0.005138	0.704264
-25.517183	-2.027916	3.021594	0.005089	0.704263
-24.668898	-2.017969	3.031590	0.004931	0.704587
-24.683825	-2.011595	3.041587	0.004935	0.704594
-24.771790	-1.996388	3.051584	0.004951	0.704592
-24.577129	-1.982268	3.061581	0.004916	0.704689
-23.710786	-2.038805	3.071578	0.004755	0.704886
-23.715477	-2.035845	3.081574	0.004756	0.704889
-23.808301	-2.017949	3.091571	0.004774	0.704891
-23.093066	-2.011028	3.101568	0.004641	0.705161
-23.224988	-1.963142	3.111565	0.004666	0.705210
-22.842638	-2.030539	3.121562	0.004595	0.705210
-22.870540	-1.957593	3.131558	0.004601	0.705346
-22.164042	-1.991553	3.141555	0.004469	0.705531
-21.985715	-2.025490	3.151552	0.004437	0.705526
-22.253613	-1.976927	3.161549	0.004487	0.705527
-21.403680	-1.961676	3.171546	0.004329	0.705861
-21.030060	-2.024870	3.181542	0.004260	0.705867
-21.097012	-2.012052	3.191539	0.004273	0.705868
-21.014658	-1.974669	3.201536	0.004258	0.705972
-20.263052	-2.027969	3.211533	0.004118	0.706134
-20.232352	-2.032792	3.221530	0.004113	0.706134
-20.507549	-1.983163	3.231526	0.004165	0.706135
-19.716396	-1.980806	3.241523	0.004018	0.706422
-19.605887	-1.988266	3.251520	0.003997	0.706446
-19.540301	-1.999190	3.261517	0.003986	0.706447
-19.036348	-2.006106	3.271514	0.003892	0.706613
-18.510538	-2.025768	3.281510	0.003795	0.706761
-18.512783	-2.025924	3.291507	0.003795	0.706759
-18.665508	-1.999178	3.301504	0.003824	0.706757
-18.079457	-1.945915	3.311501	0.003716	0.707073
-17.687821	-2.009390	3.321498	0.003643	0.707085
-17.673988	-2.009609	3.331494	0.003641	0.707089
-17.297681	-2.006929	3.341491	0.003571	0.707228
-16.914590	-1.999250	3.351488	0.003500	0.707380
-16.934440	-1.995412	3.361485	0.003504	0.707380
-16.740290	-2.027031	3.371482	0.003469	0.707385
-16.227117	-1.958991	3.381478	0.003373	0.707704
-15.967275	-2.004265	3.391475	0.003325	0.707705
-16.055701	-1.989217	3.401472	0.003342	0.707703
-15.669757	-1.960244	3.411469	0.003271	0.707898
-15.153747	-1.993370	3.421466	0.003175	0.708016
-15.262766	-1.971807	3.431462	0.003196	0.708019
-14.916147	-2.005297	3.441459	0.003132	0.708075
-14.369120	-1.962040	3.451456	0.003030	0.708357
-14.145368	-2.003063	3.461453	0.002989	0.708353
-14.174690	-1.996797	3.471450	0.002995	0.708355
-13.806369	-1.981048	3.481446	0.002927	0.708517
-13.457742	-1.979407	3.491443	0.002862	0.708644
-13.491811	-1.974206	3.501440	0.002869	0.708642
-13.289430	-1.981960	3.511437	0.002832	0.708698
-12.621601	-1.970796	3.521434	0.002708	0.708957
-12.379304	-2.012509	3.531430	0.002663	0.708960
-12.460200	-1.996191	3.541427	0.002678	0.708963
-11.976805	-1.976511	3.551424	0.002589	0.709174
-11.612884	-1.994676	3.561421	0.002521	0.709266
-11.541018	-2.005583	3.571418	0.002508	0.709270
-11.511920	-1.993246	3.581414	0.002503	0.709304
-11.037485	-1.929756	3.591411	0.002415	0.709599
-10.808757	-1.971352	3.601408	0.002373	0.709597
-10.653751	-1.999537	3.611405	0.002345	0.709595
-10.362947	-1.943047	3.621402	0.002291	0.709811
-9.854129	-1.989999	3.631398	0.002197	0.709897
-9.691435	-2.019046	3.641395	0.002167	0.709897
-9.812113	-1.975153	3.651392	0.002190	0.709941
-8.778564	-2.019725	3.661389	0.001998	0.710219
-8.763907	-2.021098	3.671386	0.001995	0.710221
-8.681071	-2.034427	3.681382	0.001980	0.710223
-8.739137	-1.960729	3.691379	0.001991	0.710349
-7.738433	-2.046511	3.701376	0.001805	0.710533
-7.864503	-2.022963	3.711373	0.001829	0.710534
-7.763658	-2.040360	3.721370	0.001811	0.710534
-7.366465	-2.027725	3.731366	0.001737	0.710700
-6.471880	-2.098223	3.741363	0.001571	0.710877
-6.920397	-2.020699	3.751360	0.001655	0.710872
-6.778538	-2.045796	3.761357	0.001629	0.710871
-6.576557	-2.009490	3.771354	0.001592	0.711015
-5.830688	-2.077021	3.781350	0.001453	0.711144
-6.127636	-2.025177	3.791347	0.001509	0.711142
-5.867051	-2.071861	3.801344	0.001461	0.711140
-5.241325	-2.037738	3.811341	0.001345	0.711430
-5.357594	-2.003791	3.821338	0.001367	0.711456
-4.928800	-2.077784	3.831334	0.001287	0.711460
-5.034436	-1.990675	3.841331	0.001307	0.711595
-3.890893	-2.110191	3.851328	0.001095	0.711762
-3.836218	-2.118537	3.861325	0.001085	0.711764
-4.048920	-2.081159	3.871322	0.001125	0.711763
-3.648416	-2.085071	3.881318	0.001051	0.711896
-3.153409	-2.074043	3.891315	0.000959	0.712093
-3.046628	-2.093633	3.901312	0.000940	0.712092
-3.204183	-2.066083	3.911309	0.000970	0.712090
-2.718889	-2.058787	3.921306	0.000880	0.712276
-2.438570	-2.050294	3.931302	0.000828	0.712391
-2.315782	-2.073090	3.941299	0.000805	0.712389
-2.181446	-2.077384	3.951296	0.000781	0.712427
-1.747075	-2.012059	3.961293	0.000700	0.712711
-1.457167	-2.061727	3.971290	0.000647	0.712714
-1.592806	-2.037221	3.981286	0.000672	0.712714
-1.300337	-1.964380	3.991283	0.000618	0.712962
-1.456320	-1.902674	4.001280	0.000648	0.713029
-1.169116	-1.953547	4.011277	0.000594	0.713028
-0.707854	-1.866839	4.021274	0.000509	0.713364
-0.924368	-1.827295	4.031270	0.000550	0.713365
-0.655256	-1.823784	4.041267	0.000500	0.713466
-0.938109	-1.678924	4.051264	0.000553	0.713654
-0.905835	-1.648330	4.061261	0.000547	0.713725
-0.710468	-1.557614	4.071258	0.000511	0.713974
-0.757492	-1.503790	4.081254	0.000520	0.714063
-0.703061	-1.404113	4.091251	0.000510	0.714280
-0.659763	-1.320127	4.101248	0.000503	0.714461
-0.516345	-1.268951	4.111245	0.000476	0.714613
-0.493030	-1.136164	4.121242	0.000472	0.714884
-0.424265	-1.073454	4.131238	0.000460	0.715032
-0.426485	-0.969996	4.141235	0.000461	0.715236
-0.189427	-0.867521	4.151232	0.000417	0.715522
-0.179356	-0.769296	4.161229	0.000415	0.715720
-0.359859	-0.625462	4.171226	0.000449	0.715940
-0.018020	-0.585293	4.181222	0.000386	0.716140
-0.103585	-0.424924	4.191219	0.000402	0.716426
-0.016776	-0.318967	4.201216	0.000386	0.716666
0.122428	-0.210811	4.211213	0.000361	0.716929
0.145245	-0.081124	4.221210	0.000357	0.717192
0.186463	0.051500	4.231206	0.000349	0.717469
0.000000	0.260691	4.241203	0.000384	0.717816

0.018772	0.879060	4.246208	0.000381	0.719043
0.051418	2.117841	4.251213	0.000374	0.721495
0.154540	3.944667	4.256218	0.000354	0.725114
0.741782	6.234168	4.261222	0.000243	0.729783
1.070913	9.084800	4.266227	0.000180	0.735417
1.558305	12.385407	4.271232	0.000088	0.741923
1.627218	16.208872	4.276237	0.000072	0.749222
2.247323	20.356717	4.281242	-0.000046	0.757242
2.648484	24.917226	4.286246	-0.000123	0.765871
2.902933	29.891953	4.291251	-0.000173	0.775114
3.458601	35.147138	4.296256	-0.000280	0.784852
3.973469	40.739114	4.301261	-0.000379	0.795059
4.603243	46.611517	4.306266	-0.000500	0.805665
5.170297	52.781838	4.311270	-0.000610	0.816632
5.721079	59.222516	4.316275	-0.000716	0.827912
6.079365	65.945105	4.321280	-0.000787	0.839459
6.550057	72.845653	4.326285	-0.000879	0.851179
8.898226	79.640542	4.331290	-0.001321	0.863110
9.826337	86.902514	4.336294	-0.001498	0.875228
10.451580	94.379267	4.341299	-0.001619	0.887439
11.525282	101.963901	4.346304	-0.001824	0.899777
12.191280	109.754203	4.351309	-0.001953	0.912157
12.889471	117.661677	4.356314	-0.002088	0.924559
13.392076	125.711025	4.361318	-0.002186	0.936960
14.221176	133.816245	4.366323	-0.002346	0.949367
14.927581	142.026677	4.371328	-0.002482	0.961737
15.575962	150.332199	4.376333	-0.002608	0.974073
16.350198	158.694053	4.381338	-0.002758	0.986367
17.180164	167.116120	4.386342	-0.002918	0.998608
17.687090	175.614410	4.391347	-0.003017	1.010729
18.354254	184.124974	4.396352	-0.003147	1.022762
19.129857	192.662222	4.401357	-0.003297	1.034716
19.351040	201.315209	4.406362	-0.003343	1.046560
20.078832	209.904914	4.411366	-0.003484	1.058305
20.596465	218.553950	4.416371	-0.003586	1.069950
21.042361	227.212534	4.421376	-0.003674	1.081466
21.701063	235.839192	4.426381	-0.003803	1.092866
22.350987	244.483031	4.431386	-0.003929	1.104169
23.028612	253.128803	4.436390	-0.004061	1.115365
23.505928	261.790652	4.441395	-0.004155	1.126427
24.074423	270.456437	4.446400	-0.004266	1.137405
24.635561	279.108608	4.451405	-0.004376	1.148259
25.168119	287.772447	4.456410	-0.004481	1.159020
25.813308	296.378603	4.461414	-0.004606	1.169635
26.147959	305.026101	4.466419	-0.004674	1.180140
26.915344	313.610643	4.471424	-0.004822	1.190565
27.238844	322.229079	4.476429	-0.004888	1.200850
28.018169	330.785758	4.481434	-0.005038	1.211066
28.603775	339.358795	4.486438	-0.005153	1.221177
29.122278	347.939188	4.491443	-0.005255	1.231200
29.463111	356.513764	4.496448	-0.005324	1.241100
30.036056	365.017607	4.501453	-0.005436	1.250887
30.650471	373.521450	4.506458	-0.005555	1.260605
31.440231	381.984883	4.511462	-0.005708	1.270236
32.352846	390.417279	4.516467	-0.005883	1.279783
33.113959	398.884359	4.521472	-0.006030	1.289269
33.287083	407.421601	4.526477	-0.006068	1.298654
33.943920	415.897826	4.531482	-0.006195	1.307994
34.627892	424.437987	4.536486	-0.006328	1.317341
35.021865	432.861948	4.541491	-0.006407	1.326445
35.526347	441.293120	4.546496	-0.006506	1.335515
36.041273	449.681814	4.551501	-0.006607	1.344480
36.741609	458.063838	4.556506	-0.006743	1.353411
37.353222	466.425711	4.561510	-0.006862	1.362246
37.812878	474.815985	4.566515	-0.006953	1.371028
38.334246	483.198936	4.571520	-0.007055	1.379757
38.448897	491.622540	4.576525	-0.007082	1.388403
38.847931	500.014217	4.581530	-0.007161	1.397011
39.687852	508.280951	4.586534	-0.007323	1.405514
40.018162	516.656606	4.591539	-0.007390	1.413990
40.394546	525.006547	4.596544	-0.007465	1.422397
40.803581	533.338415	4.601549	-0.007546	1.430742
41.046658	541.700840	4.606554	-0.007597	1.439042
41.578753	549.980211	4.611558	-0.007701	1.447259
41.914004	558.320594	4.616563	-0.007769	1.455457
42.785942	566.546220	4.621568	-0.007936	1.463584
42.883368	574.925641	4.626573	-0.007960	1.471691
43.342368	583.225569	4.631578	-0.008050	1.479735
43.833245	591.478293	4.636582	-0.008147	1.487694
44.516767	599.714617	4.641587	-0.008279	1.495626
45.083505	607.965334	4.646592	-0.008390	1.503511
45.535520	616.236087	4.651597	-0.008480	1.511356
45.769633	624.538762	4.656602	-0.008528	1.519156
46.329974	632.766320	4.661606	-0.008638	1.526897
46.757080	641.031839	4.666611	-0.008723	1.534613
47.253422	649.279900	4.671616	-0.008820	1.542285
47.595777	657.542248	4.676621	-0.008889	1.549908
48.070063	665.800210	4.681626	-0.008983	1.557510
48.549866	673.999302	4.686630	-0.009077	1.565022
48.981454	682.246033	4.691635	-0.009163	1.572534
49.558231	690.450523	4.696640	-0.009275	1.579994
49.832068	698.690159	4.701645	-0.009331	1.587405
50.191573	706.946820	4.706650	-0.009403	1.594810
50.604615	715.150241	4.711654	-0.009485	1.602141
51.081155	723.356219	4.716659	-0.009579	1.609449
51.645402	731.570184	4.721664	-0.009690	1.616744
51.849637	739.794768	4.726669	-0.009733	1.623964
52.441657	748.022991	4.731674	-0.009848	1.631210
52.807448	756.262365	4.736678	-0.009921	1.638402
53.033114	764.446534	4.741683	-0.009969	1.645495
53.419917	772.667776	4.746688	-0.010046	1.652612
54.000797	780.808843	4.751693	-0.010159	1.659655
54.408001	788.994954	4.756698	-0.010240	1.666684
54.643928	797.225585	4.761702	-0.010289	1.673698
55.136708	805.368856	4.766707	-0.010386	1.680643
55.752655	813.517026	4.771712	-0.010506	1.687580
56.134741	821.705023	4.776717	-0.010582	1.694490
56.578298	829.881942	4.781722	-0.010670	1.701371
57.006221	838.055786	4.786726	-0.010755	1.708220
57.163397	846.305940	4.791731	-0.010789	1.715069
57.241220	854.493620	4.796736	-0.010809	1.721829
57.765805	862.619031	4.801741	-0.010911	1.728569
58.306628	870.778577	4.806746	-0.011017	1.735313
58.613064	878.947483	4.811750	-0.011079	1.742008
58.810221	887.133281	4.816755	-0.011121	1.748677
59.301079	895.292277	4.821760	-0.011218	1.755337
59.916150	903.393302	4.826765	-0.011337	1.761940
59.952323	911.602752	4.831770	-0.011349	1.768532
60.348596	919.771188	4.836774	-0.011428	1.775112
60.689117	927.915415	4.841779	-0.011497	1.781642
60.983060	936.089041	4.846784	-0.011557	1.788165
61.542756	944.259716	4.851789	-0.011666	1.794694
62.057864	952.365609	4.856794	-0.011767	1.801144
62.524299	960.490682	4.861798	-0.011859	1.807579
62.946638	968.625812	4.866803	-0.011943	1.813994
63.641210	976.730704	4.871808	-0.012077	1.820395
63.775103	984.897072	4.876813	-0.012107	1.826754
64.089102	993.077057	4.881818	-0.012171	1.833123
64.716043	1001.178512	4.886822	-0.012293	1.839447
65.146216	1009.294322	4.891827	-0.012378	1.845736
65.441186	1017.479587	4.896832	-0.012438	1.852041
65.808565	1025.608640	4.901837	-0.012511	1.858291
66.311083	1033.737356	4.906842	-0.012610	1.864534
66.520860	1041.912953	4.911846	-0.012654	1.870759
66.846837	1050.066001	4.916851	-0.012720	1.876959
67.352164	1058.163797	4.921856	-0.012819	1.883117
67.605955	1066.287915	4.926861	-0.012871	1.889246
68.043240	1074.429379	4.931866	-0.012958	1.895389
68.533245	1082.519672	4.936870	-0.013054	1.901480
68.986290	1090.629772	4.941875	-0.013144	1.907562
69.298495	1098.797200	4.946880	-0.013207	1.913652
69.610356	1106.905936	4.951885	-0.013270	1.919678
70.153975	1114.994423	4.956890	-0.013376	1.925696
70.304509	1123.169040	4.961894	-0.013410	1.931715
70.721077	1131.280555	4.966899	-0.013492	1.937699
71.178211	1139.383574	4.971904	-0.013582	1.943662
71.468342	1147.515269	4.976909	-0.013642	1.949609
71.663742	1155.702225	4.981914	-0.013683	1.955568
71.961911	1163.790413	4.986918	-0.013744	1.961449
72.253047	1171.877961	4.991923	-0.013803	1.967311
72.708681	1180.000558	4.996928	-0.013893	1.973198
72.837109	1188.122899	5.001933	-0.013922	1.979032
73.256147	1196.200658	5.006938	-0.014005	1.984848
73.563936	1204.308062	5.011942	-0.014067	1.990656
73.797834	1212.438959	5.016947	-0.014116	1.996457
74.254184	1220.517221	5.021952	-0.014206	2.002226
74.584963	1228.609015	5.026957	-0.014273	2.007975
74.878872	1236.737075	5.031962	-0.014333	2.013730
75.168687	1244.844725	5.036966	-0.014392	2.019453
75.506996	1252.929850	5.041971	-0.014460	2.025149
76.016370	1261.047739	5.046976	-0.014560	2.030869
76.284138	1269.163003	5.051981	-0.014615	2.036547
76.614364	1277.244462	5.056986	-0.014681	2.042192
77.018746	1285.338579	5.061990	-0.014762	2.047837
77.137108	1293.473997	5.066995	-0.014789	2.053466
77.639404	1301.551793	5.072000	-0.014887	2.059079
77.942452	1309.639987	5.077005	-0.014949	2.064664
78.293787	1317.758806	5.082010	-0.015019	2.070259
78.338253	1325.910084	5.087014	-0.015033	2.075831
78.764292	1333.956143	5.092019	-0.015117	2.081354
79.220448	1342.033578	5.097024	-0.015207	2.086886
79.462761	1350.136893	5.102029	-0.015257	2.092400
79.644774	1358.271694	5.107034	-0.015296	2.097915
80.037834	1366.333248	5.112038	-0.015375	2.103387
80.206135	1374.446304	5.117043	-0.015411	2.108857
80.455421	1382.625286	5.122048	-0.015463	2.114365
80.923476	1390.632039	5.127053	-0.015555	2.119765
81.250891	1398.700697	5.132058	-0.015621	2.125179
81.552620	1406.799058	5.137062	-0.015682	2.130596
81.986554	1414.857592	5.142067	-0.015768	2.135985
82.411201	1422.934614	5.147072	-0.015852	2.141372
82.377166	1431.047621	5.152077	-0.015851	2.146726
82.622197	1439.156599	5.157082	-0.015901	2.152090
83.051169	1447.227607	5.162086	-0.015986	2.157433
83.279431	1455.290368	5.167091	-0.016034	2.162738
83.837124	1463.354852	5.172096	-0.016143	2.168063
84.160860	1471.445565	5.177101	-0.016208	2.173369
84.464516	1479.547149	5.182106	-0.016270	2.178668
84.733711	1487.636741	5.187110	-0.016325	2.183943
84.968786	1495.732593	5.192115	-0.016374	2.189205
85.549820	1503.833512	5.197120	-0.016487	2.194491
85.640856	1511.916440	5.202125	-0.016509	2.199707
86.048436	1519.950130	5.207130	-0.016590	2.204907
86.778906	1527.979523	5.212134	-0.016731	2.210122
87.300205	1536.047360	5.217139	-0.016833	2.215330
87.633654	1544.149224	5.222144	-0.016900	2.220531
88.090968	1552.208279	5.227149	-0.016991	2.225703
88.535386	1560.301025	5.232154	-0.017078	2.230884
88.586654	1568.438102	5.237158	-0.017093	2.236045
88.904564	1576.495963	5.242163	-0.017157	2.241168
89.290218	1584.575928	5.247168	-0.017234	2.246299
89.552893	1592.671932	5.252173	-0.017288	2.251418
89.770514	1600.771678	5.257178	-0.017334	2.256523
90.233364	1608.817194	5.262182	-0.017425	2.261605
90.435679	1616.901551	5.267187	-0.017468	2.266676
90.665881	1625.050162	5.272192	-0.017516	2.271778
91.018178	1633.137595	5.277197	-0.017586	2.276842
91.168323	1641.187171	5.282202	-0.017619	2.281853
91.552048	1649.228883	5.287206	-0.017696	2.286868
91.894256	1657.283380	5.292211	-0.017765	2.291877
91.980176	1665.398358	5.297216	-0.017786	2.296890
92.258263	1673.447610	5.302221	-0.017843	2.301868
92.390938	1681.518413	5.307226	-0.017872	2.306836
92.866658	1689.580622	5.312230	-0.017966	2.311817
93.041254	1697.652443	5.317235	-0.018004	2.316768
93.415875	1705.695895	5.322240	-0.018078	2.321708
93.637713	1713.754750	5.327245	-0.018125	2.326634
94.005911	1721.827621	5.332250	-0.018198	2.331570
94.281017	1729.917898	5.337254	-0.018255	2.336498
94.477578	1737.962523	5.342259	-0.018296	2.341382
94.981326	1746.010885	5.347264	-0.018395	2.346283
95.063516	1754.149608	5.352269	-0.018416	2.351193
95.543446	1762.204838	5.357274	-0.018510	2.356076
95.964330	1770.247325	5.362278	-0.018593	2.360935
96.156753	1778.294952	5.367283	-0.018634	2.365770
96.620139	1786.359559	5.372288	-0.018726	2.370626
96.718007	1794.457424	5.377293	-0.018749	2.375463
97.200659	1802.496571	5.382298	-0.018844	2.380286
97.245171	1810.591632	5.387302	-0.018857	2.385097
97.208651	1818.682821	5.392307	-0.018855	2.389890
97.764407	1826.737736	5.397312	-0.018964	2.394699
98.132713	1834.764632	5.402317	-0.019038	2.399467
98.282707	1842.829419	5.407322	-0.019071	2.404230
98.735092	1850.885737	5.412326	-0.019160	2.409002
99.052903	1858.944007	5.417331	-0.019224	2.413756
99.163008	1867.052348	5.422336	-0.019250	2.418513
99.615343	1875.072575	5.427341	-0.019339	2.423236
100.070701	1883.117995	5.432346	-0.019429	2.427965
100.209654	1891.279447	5.437350	-0.019460	2.432727
100.509637	1899.335721	5.442355	-0.019521	2.437432
100.657546	1907.378763	5.447360	-0.019553	2.442108
101.047232	1915.407142	5.452365	-0.019631	2.446784
101.244130	1923.486200	5.457370	-0.019673	2.451467
101.591652	1931.551062	5.462374	-0.019742	2.456144
101.937553	1939.589118	5.467379	-0.019812	2.460796
102.238337	1947.635459	5.472384	-0.019873	2.465441
102.387392	1955.715896	5.477389	-0.019906	2.470085
102.767985	1963.770812	5.482394	-0.019982	2.474723
103.007046	1971.824776	5.487398	-0.020031	2.479341
103.008149	1979.877984	5.492403	-0.020036	2.483933
103.403709	1987.938564	5.497408	-0.020115	2.488549
103.662758	1996.007580	5.502413	-0.020168	2.493152
103.893771	2004.066648	5.507418	-0.020217	2.497738
104.084589	2012.135109	5.512422	-0.020257	2.502318
104.329596	2020.155344	5.517427	-0.020308	2.506866
104.542575	2028.280608	5.522432	-0.020353	2.511463
104.680186	2036.356199	5.527437	-0.020383	2.516018
104.942976	2044.374270	5.532442	-0.020437	2.520542
105.244653	2052.397752	5.537446	-0.020498	2.525063
105.510344	2060.421718	5.542451	-0.020553	2.529574
105.765987	2068.509556	5.547456	-0.020606	2.534112
106.232052	2076.534784	5.552461	-0.020697	2.538621
106.385710	2084.583804	5.557466	-0.020731	2.543114
106.840593	2092.648750	5.562470	-0.020821	2.547629
107.364242	2100.669994	5.567475	-0.020923	2.552116
107.886706	2108.734329	5.572480	-0.021026	2.556619
108.055105	2116.793341	5.577485	-0.021062	2.561086
108.154056	2124.854935	5.582490	-0.021086	2.565542
108.368464	2132.939007	5.587494	-0.021131	2.570011
108.632878	2140.987237	5.592499	-0.021185	2.574456
109.107657	2149.030181	5.597504	-0.021278	2.578904
109.596468	2157.053620	5.602509	-0.021374	2.583335
109.813877	2165.122054	5.607514	-0.021420	2.587765
110.223717	2173.286754	5.612518	-0.021501	2.592252
110.586082	2181.388703	5.617523	-0.021574	2.596694
111.008748	2189.373225	5.622528	-0.021658	2.601069
110.899242	2197.437521	5.627533	-0.021642	2.605443
111.250794	2205.436600	5.632538	-0.021713	2.609806
111.811779	2213.487006	5.637542	-0.021822	2.614204
111.813071	2221.519924	5.642547	-0.021827	2.618547
111.936164	2229.566724	5.647552	-0.021855	2.622898
112.258131	2237.604974	5.652557	-0.021920	2.627251
112.626597	2245.638814	5.657562	-0.021994	2.631598
112.828862	2253.731968	5.662566	-0.022037	2.635957
113.016897	2261.749785	5.667571	-0.022077	2.640269
113.177496	2269.804628	5.672576	-0.022112	2.644591
113.498564	2277.836100	5.677581	-0.022177	2.648904
113.858609	2285.901266	5.682586	-0.022249	2.653231
114.158810	2293.945787	5.687590	-0.022310	2.657535
114.398736	2301.987984	5.692595	-0.022359	2.661828
114.616126	2310.060185	5.697600	-0.022405	2.666128
114.985161	2318.095848	5.702605	-0.022479	2.670411
115.131227	2326.188274	5.707610	-0.022511	2.674703
115.225658	2334.253937	5.712614	-0.022534	2.678971
115.487478	2342.238798	5.717619	-0.022587	2.683200
116.010643	2350.263526	5.722624	-0.022690	2.687460
116.143333	2358.339552	5.727629	-0.022720	2.691715
116.314373	2366.396444	5.732634	-0.022756	2.695956
116.747069	2374.441778	5.737638	-0.022842	2.700201
116.946830	2382.445649	5.742643	-0.022884	2.704403
117.038047	2390.546266	5.747648	-0.022906	2.708641
117.569040	2398.557837	5.752653	-0.023010	2.712855
117.749992	2406.615651	5.757658	-0.023049	2.717063
117.908427	2414.650915	5.762662	-0.023084	2.721252
118.171053	2422.671196	5.767667	-0.023137	2.725434
118.362523	2430.729294	5.772672	-0.023178	2.729624
118.586144	2438.813571	5.777677	-0.023225	2.733823
118.550144	2446.880169	5.782682	-0.023223	2.737990
118.929986	2454.900709	5.787686	-0.023299	2.742153
118.940392	2462.938548	5.792691	-0.023306	2.746296
119.443289	2470.990505	5.797696	-0.023405	2.750470
119.640734	2479.126868	5.802701	-0.023447	2.754662
119.616207	2487.137426	5.807706	-0.023447	2.758770
119.975750	2495.155056	5.812710	-0.023519	2.762899
120.218833	2503.161895	5.817715	-0.023569	2.767008
120.505401	2511.214845	5.822720	-0.023628	2.771138
120.571621	2519.290416	5.827725	-0.023645	2.775260
120.703240	2527.296162	5.832730	-0.023675	2.779344
121.098767	2535.328493	5.837734	-0.023753	2.783452
121.322761	2543.364559	5.842739	-0.023800	2.787545
121.639491	2551.424605	5.847744	-0.023864	2.791649
121.960791	2559.473949	5.852749	-0.023929	2.795742
122.223636	2567.480229	5.857754	-0.023983	2.799804
122.593222	2575.510101	5.862758	-0.024057	2.803879
122.708265	2583.558904	5.867763	-0.024083	2.807942
123.027567	2591.632549	5.872768	-0.024148	2.812023
123.025033	2599.710956	5.877773	-0.024152	2.816082
123.225600	2607.714836	5.882778	-0.024195	2.820110
123.522175	2615.751078	5.887782	-0.024255	2.824154
123.717727	2623.795575	5.892787	-0.024296	2.828190
123.834066	2631.889487	5.897792	-0.024323	2.832240
124.161653	2639.939047	5.902797	-0.024389	2.836275
124.257925	2647.935015	5.907802	-0.024412	2.840264
124.468201	2655.972039	5.912806	-0.024456	2.844274
124.467712	2664.004806	5.917811	-0.024461	2.848265
124.744176	2672.060952	5.922816	-0.024518	2.852277
125.031117	2680.095253	5.927821	-0.024576	2.856273
125.189086	2688.132783	5.932826	-0.024611	2.860258
125.567963	2696.154211	5.937830	-0.024686	2.864241
125.732949	2704.200297	5.942835	-0.024722	2.868220
125.980294	2712.271241	5.947840	-0.024773	2.872209
126.291122	2720.318495	5.952845	-0.024836	2.876185
126.532876	2728.328822	5.957850	-0.024886	2.880134
126.790121	2736.367017	5.962854	-0.024939	2.884091
126.982003	2744.404553	5.967859	-0.024980	2.888039
127.296396	2752.488741	5.972864	-0.025043	2.892011
127.598436	2760.535716	5.977869	-0.025105	2.895959
127.669226	2768.551600	5.982874	-0.025123	2.899874
128.163114	2776.569376	5.987878	-0.025220	2.903807
128.267306	2784.607951	5.992883	-0.025244	2.907724
128.592492	2792.696070	5.997888	-0.025310	2.911671
128.717099	2800.811631	6.002893	-0.025338	2.915616
129.124683	2808.737615	6.007898	-0.025419	2.919478
129.232151	2816.787281	6.012902	-0.025444	2.923380
129.396104	2824.769182	6.017907	-0.025480	2.927246
129.872694	2832.814946	6.022912	-0.025574	2.931154
130.183366	2840.876848	6.027917	-0.025636	2.935057
130.134938	2848.916068	6.032922	-0.025632	2.938924
130.489948	2856.937601	6.037926	-0.025704	2.942798
130.794582	2864.965608	6.042931	-0.025765	2.946668
130.869438	2873.036392	6.047936	-0.025784	2.950542
131.100032	2881.084028	6.052941	-0.025832	2.954407
131.392245	2889.086687	6.057946	-0.025892	2.958249
131.736851	2897.131553	6.062950	-0.025961	2.962109
131.874617	2905.147773	6.067955	-0.025992	2.965939
132.248395	2913.181240	6.072960	-0.026066	2.969785
132.539391	2921.258492	6.077965	-0.026126	2.973642
132.656753	2929.280794	6.082970	-0.026152	2.977460
133.186304	2937.292504	6.087974	-0.026256	2.981288
133.399536	2945.304333	6.092979	-0.026301	2.985095
133.548237	2953.384859	6.097984	-0.026334	2.988927
133.832539	2961.477308	6.102989	-0.026392	2.992766
134.024805	2969.498729	6.107994	-0.026432	2.996562
134.251078	2977.530808	6.112998	-0.026480	3.000360
134.256911	2985.535422	6.118003	-0.026486	3.004129
134.680131	2993.555937	6.123008	-0.026569	3.007922
134.770367	3001.633802	6.128013	-0.026591	3.011720
134.832700	3009.682223	6.133018	-0.026608	3.015498
135.291947	3017.671842	6.138022	-0.026699	3.019263
135.457874	3025.699693	6.143027	-0.026734	3.023028
135.498927	3033.750011	6.148032	-0.026747	3.026792
135.685921	3041.803201	6.153037	-0.026787	3.030559
136.002880	3049.838924	6.158042	-0.026851	3.034320
136.175117	3057.875658	6.163046	-0.026888	3.038070
136.024009	3065.920990	6.168051	-0.026865	3.041804
136.504251	3073.918903	6.173056	-0.026960	3.045541
136.812260	3081.944677	6.178061	-0.027022	3.049278
136.875199	3089.995601	6.183066	-0.027039	3.053011
137.308859	3098.035168	6.188070	-0.027124	3.056752
137.467558	3106.062340	6.193075	-0.027159	3.060469
137.612043	3114.089987	6.198080	-0.027191	3.064181
137.747366	3122.152780	6.203085	-0.027221	3.067904
138.243708	3130.195381	6.208090	-0.027319	3.071630
138.613237	3138.282668	6.213094	-0.027393	3.075367
138.602036	3146.284715	6.218099	-0.027396	3.079042
138.681104	3154.297376	6.223104	-0.027415	3.082721
139.063743	3162.314134	6.228109	-0.027492	3.086412
138.965387	3170.359284	6.233114	-0.027478	3.090090
139.184168	3178.417510	6.238118	-0.027524	3.093784
139.388323	3186.425380	6.243123	-0.027567	3.097449
139.595125	3194.440526	6.248128	-0.027611	3.101114
139.853137	3202.450525	6.253133	-0.027664	3.104774
140.097246	3210.495538	6.258138	-0.027714	3.108445
140.472148	3218.559809	6.263142	-0.027789	3.112127
140.560531	3226.612846	6.268147	-0.027811	3.115786
140.797044	3234.593816	6.273152	-0.027860	3.119414
141.043863	3242.620435	6.278157	-0.027911	3.123060
141.138111	3250.671000	6.283162	-0.027933	3.126705
141.201382	3258.713335	6.288166	-0.027950	3.130341
141.519147	3266.724694	6.293171	-0.028014	3.133970
141.828612	3274.787218	6.298176	-0.028077	3.137617
141.913898	3282.827213	6.303181	-0.028098	3.141240
142.110168	3290.819792	6.308186	-0.028139	3.144843
142.507223	3298.853437	6.313190	-0.028218	3.148469
142.506447	3306.915952	6.318195	-0.028223	3.152085
142.724522	3315.007508	6.323200	-0.028269	3.155721
142.901833	3322.998019	6.328205	-0.028307	3.159305
143.152258	3330.982207	6.333210	-0.028359	3.162885
143.451411	3339.015616	6.338214	-0.028419	3.166485
143.537838	3347.051606	6.343219	-0.028440	3.170073
143.805014	3355.100320	6.348224	-0.028495	3.173671
144.033498	3363.144490	6.353229	-0.028543	3.177261
144.101787	3371.152859	6.358234	-0.028561	3.180823
144.509267	3379.134860	6.363238	-0.028641	3.184385
144.762201	3387.184484	6.368243	-0.028694	3.187966
144.742803	3395.267928	6.373248	-0.028695	3.191546
145.057669	3403.329247	6.378253	-0.028759	3.195127
145.110550	3411.338511	6.383258	-0.028774	3.198669
145.468733	3419.363040	6.388262	-0.028845	3.202228
145.664905	3427.357510	6.393267	-0.028887	3.205762
145.881381	3435.400817	6.398272	-0.028932	3.209314
146.065522	3443.471821	6.403277	-0.028972	3.212874
146.333576	3451.475742	6.408282	-0.029027	3.216403
146.474690	3459.508362	6.413286	-0.029058	3.219936
146.736278	3467.510793	6.418291	-0.029112	3.223457
147.023495	3475.541096	6.423296	-0.029170	3.226987
147.306015	3483.607189	6.428301	-0.029228	3.230528
147.338747	3491.688436	6.433306	-0.029239	3.234062
147.599441	3499.672912	6.438310	-0.029292	3.237560
147.742289	3507.707897	6.443315	-0.029324	3.241070
148.032334	3515.674937	6.448320	-0.029383	3.244553
148.316153	3523.729487	6.453325	-0.029441	3.248071
148.399848	3531.756072	6.458330	-0.029462	3.251564
148.777571	3539.796609	6.463334	-0.029537	3.255071
149.045864	3547.814311	6.468339	-0.029592	3.258560
149.212152	3555.851545	6.473344	-0.029628	3.262050
149.282518	3563.883886	6.478349	-0.029646	3.265530
149.415457	3571.898174	6.483354	-0.029676	3.269001
149.625253	3579.971168	6.488358	-0.029720	3.272497
149.890808	3587.989198	6.493363	-0.029774	3.275967
150.138610	3595.985594	6.498368	-0.029826	3.279424
150.253296	3604.035253	6.503373	-0.029852	3.282895
150.390346	3612.076222	6.508378	-0.029883	3.286359
150.603247	3620.108004	6.513382	-0.029927	3.289818
150.783215	3628.158591	6.518387	-0.029966	3.293281
150.961231	3636.190966	6.523392	-0.030004	3.296732
151.503680	3644.185341	6.528397	-0.030110	3.300177
151.719319	3652.183247	6.533402	-0.030155	3.303608
151.853390	3660.240699	6.538406	-0.030185	3.307057
151.969846	3668.263580	6.543411	-0.030212	3.310487
152.252403	3676.341603	6.548416	-0.030270	3.313943
152.259681	3684.378561	6.553421	-0.030276	3.317368
152.479385	3692.360286	6.558426	-0.030322	3.320774
153.016855	3700.325215	6.563430	-0.030427	3.324181
153.093918	3708.371471	6.568435	-0.030446	3.327602
153.169997	3716.433498	6.573440	-0.030466	3.331026
153.576275	3724.466814	6.578445	-0.030546	3.334446
153.536884	3732.484123	6.583450	-0.030544	3.337840
153.848407	3740.546148	6.588454	-0.030607	3.341262
153.904648	3748.519822	6.593459	-0.030623	3.344634
154.106669	3756.579915	6.598464	-0.030665	3.348044
154.384878	3764.627653	6.603469	-0.030722	3.351448
154.336757	3772.676349	6.608474	-0.030718	3.354837
154.924775	3780.649331	6.613478	-0.030833	3.358214
155.032766	3788.721728	6.618483	-0.030858	3.361612
155.054605	3796.707872	6.623488	-0.030867	3.364968
155.195864	3804.758763	6.628493	-0.030898	3.368351
155.652824	3812.769216	6.633498	-0.030988	3.371725
155.439221	3820.866760	6.638502	-0.030954	3.375108
155.556555	3828.870994	6.643507	-0.030980	3.378461
155.666070	3836.886146	6.648512	-0.031006	3.381815
156.037308	3844.885639	6.653517	-0.031080	3.385168
155.824242	3852.930661	6.658522	-0.031045	3.388516
156.091643	3860.990246	6.663526	-0.031100	3.391884
156.443817	3869.058344	6.668531	-0.031171	3.395254
156.607250	3877.031804	6.673536	-0.031206	3.398576
156.932164	3885.043980	6.678541	-0.031272	3.401916
157.155910	3893.016199	6.683546	-0.031319	3.405232
157.489832	3901.066970	6.688550	-0.031386	3.408582
157.490899	3909.127117	6.693555	-0.031391	3.411921
157.790663	3917.124336	6.698560	-0.031452	3.415240
157.952505	3925.177924	6.703565	-0.031487	3.418575
157.959990	3933.185654	6.708570	-0.031493	3.421883
158.382371	3941.161654	6.713574	-0.031577	3.425188
158.530084	3949.228763	6.718579	-0.031610	3.428518
158.542080	3957.280031	6.723584	-0.031617	3.431834
158.669206	3965.345622	6.728589	-0.031646	3.435156
159.005189	3973.301725	6.733594	-0.031713	3.438438
159.373010	3981.330700	6.738598	-0.031787	3.441747
159.375474	3989.358427	6.743603	-0.031792	3.445040
159.524797	3997.362124	6.748608	-0.031825	3.448325
159.768044	4005.443752	6.753613	-0.031875	3.451642
160.113405	4013.460130	6.758618	-0.031945	3.454932
160.410209	4021.468351	6.763622	-0.032005	3.458214
160.801717	4029.481313	6.768627	-0.032083	3.461498
160.823055	4037.513331	6.773632	-0.032092	3.464775
161.042767	4045.552456	6.778637	-0.032138	3.468057
161.176972	4053.609189	6.783642	-0.032168	3.471341
161.582106	4061.643640	6.788646	-0.032248	3.474622
161.631791	4069.667934	6.793651	-0.032263	3.477884
161.833433	4077.667767	6.798656	-0.032305	3.481138
162.153795	4085.685842	6.803661	-0.032370	3.484399
162.067247	4093.714315	6.808666	-0.032359	3.487649
162.340747	4101.722749	6.813670	-0.032415	3.490900
162.532169	4109.786915	6.818675	-0.032456	3.494167
162.799033	4117.790210	6.823680	-0.032510	3.497409
162.932824	4125.823037	6.828685	-0.032540	3.500655
163.187146	4133.798254	6.833690	-0.032593	3.503879
163.627028	4141.852607	6.838694	-0.032679	3.507138
163.652311	4149.906374	6.843699	-0.032689	3.510381
163.723294	4157.938449	6.848704	-0.032707	3.513613
163.977991	4165.970819	6.853709	-0.032760	3.516848
164.203062	4173.949954	6.858714	-0.032807	3.520058
164.472593	4181.969684	6.863718	-0.032862	3.523282
164.595514	4190.016662	6.868723	-0.032890	3.526510
164.722018	4198.016962	6.873728	-0.032919	3.529716
164.987537	4206.078863	6.878733	-0.032973	3.532948
165.102108	4214.123755	6.883738	-0.032999	3.536166
165.432697	4222.112761	6.888742	-0.033066	3.539365
165.773271	4230.156954	6.893747	-0.033134	3.542584
165.862578	4238.167162	6.898752	-0.033156	3.545778
166.095445	4246.205257	6.903757	-0.033205	3.548985
166.007141	4254.297534	6.908762	-0.033193	3.552201
166.237690	4262.384325	6.913766	-0.033241	3.555422
166.559543	4270.320718	6.918771	-0.033306	3.558582
166.553531	4278.333535	6.923776	-0.033310	3.561760
166.760273	4286.313331	6.928781	-0.033353	3.564929
166.957020	4294.327096	6.933786	-0.033395	3.568108
167.139059	4302.392611	6.938790	-0.033434	3.571304
167.152580	4310.427241	6.943795	-0.033442	3.574480
167.279113	4318.448888	6.948800	-0.033470	3.577651
167.817288	4326.429436	6.953805	-0.033575	3.580815
167.874153	4334.415913	6.958810	-0.033591	3.583965
167.942658	4342.493460	6.963814	-0.033609	3.587148
168.255012	4350.508953	6.968819	-0.033672	3.590311
168.219701	4358.565529	6.973824	-0.033671	3.593477
168.416174	4366.616470	6.978829	-0.033712	3.596645
168.271232	4374.569422	6.983834	-0.033690	3.599762
168.633254	4382.586059	6.988838	-0.033763	3.602916
168.874579	4390.610546	6.993843	-0.033813	3.606066
168.814362	4398.619781	6.998848	-0.033806	3.609199
169.344709	4406.669832	7.003853	-0.033910	3.612362
169.577112	4414.679568	7.008858	-0.033958	3.615498
169.702075	4422.727170	7.013862	-0.033987	3.618643
169.964068	4430.744946	7.018867	-0.034041	3.621778
170.233808	4438.734785	7.023872	-0.034096	3.624899
170.468153	4446.777436	7.028877	-0.034145	3.628037
170.527957	4454.829736	7.033882	-0.034161	3.631171
170.840755	4462.913167	7.038886	-0.034224	3.634321
171.037353	4470.905679	7.043891	-0.034266	3.637431
170.745696	4478.912425	7.048896	-0.034216	3.640530
171.015263	4486.944253	7.053901	-0.034272	3.643651
171.185763	4494.923003	7.058906	-0.034308	3.646746
171.493025	4502.933909	7.063910	-0.034371	3.649854
171.666068	4511.009457	7.068915	-0.034408	3.652982
171.915200	4519.030217	7.073920	-0.034459	3.656087
172.123217	4527.057483	7.078925	-0.034503	3.659191
172.131328	4535.062339	7.083930	-0.034510	3.662279
172.444406	4543.088133	7.088934	-0.034573	3.665380
172.711526	4551.119111	7.093939	-0.034628	3.668479
172.754378	4559.160759	7.098944	-0.034641	3.671574
172.950327	4567.215177	7.103949	-0.034682	3.674675
172.952904	4575.210571	7.108954	-0.034688	3.677746
173.073735	4583.218589	7.113958	-0.034715	3.680822
173.315662	4591.187011	7.118963	-0.034765	3.683884
173.486314	4599.245992	7.123968	-0.034802	3.686975
173.816709	4607.279207	7.128973	-0.034869	3.690059
173.925245	4615.311899	7.133978	-0.034894	3.693133
174.090940	4623.350029	7.138982	-0.034930	3.696209
174.436189	4631.342244	7.143987	-0.034999	3.699269
174.685708	4639.338498	7.148992	-0.035051	3.702326
174.788996	4647.377241	7.153997	-0.035075	3.705393
175.314640	4655.378811	7.159002	-0.035178	3.708453
175.224657	4663.475597	7.164006	-0.035166	3.711532
175.252551	4671.580483	7.169011	-0.035176	3.714615
175.512655	4679.546431	7.174016	-0.035230	3.717647
175.848328	4687.538828	7.179021	-0.035297	3.720689
175.904600	4695.492425	7.184026	-0.035313	3.723708
176.115694	4703.505245	7.189030	-0.035357	3.726749
176.344736	4711.535939	7.194035	-0.035405	3.729796
176.502551	4719.583610	7.199040	-0.035439	3.732844
176.702055	4727.617947	7.204045	-0.035481	3.735886
177.108393	4735.585511	7.209050	-0.035562	3.738906
177.289007	4743.650038	7.214054	-0.035601	3.741954
177.308535	4751.660107	7.219059	-0.035609	3.744975
177.616006	4759.648705	7.224064	-0.035672	3.747992
177.623262	4767.762975	7.229069	-0.035678	3.751048
177.630657	4775.785065	7.234074	-0.035684	3.754066
177.982736	4783.783124	7.239078	-0.035755	3.757080
178.184760	4791.786226	7.244083	-0.035798	3.760091
178.275521	4799.807682	7.249088	-0.035820	3.763103
178.368850	4807.836286	7.254093	-0.035842	3.766116
178.438748	4815.852795	7.259098	-0.035860	3.769121
178.825492	4823.898127	7.264102	-0.035937	3.772142
179.006133	4831.947587	7.269107	-0.035976	3.775157
179.286284	4839.960771	7.274112	-0.036033	3.778159
179.743122	4847.972295	7.279117	-0.036123	3.781161
179.779283	4855.949602	7.284122	-0.036135	3.784139
179.667713	4863.997362	7.289126	-0.036119	3.787137
179.886467	4872.040919	7.294131	-0.036165	3.790139
179.985027	4880.079666	7.299136	-0.036188	3.793134
180.274888	4888.147870	7.304141	-0.036247	3.796142
180.450143	4896.078149	7.309146	-0.036285	3.799093
180.506643	4904.120075	7.314150	-0.036300	3.802081
180.725138	4912.072985	7.319155	-0.036346	3.805038
180.855344	4920.123268	7.324160	-0.036375	3.808026
180.936967	4928.169290	7.329165	-0.036396	3.811009
181.091185	4936.182000	7.334170	-0.036429	3.813979
181.340605	4944.240245	7.339174	-0.036481	3.816965
181.634141	4952.194218	7.344179	-0.036541	3.819912
181.525388	4960.234321	7.349184	-0.036525	3.822879
181.736959	4968.234292	7.354189	-0.036570	3.825836
181.865152	4976.264806	7.359194	-0.036599	3.828801
182.158058	4984.320169	7.364198	-0.036658	3.831775
182.292815	4992.350211	7.369203	-0.036688	3.834735
182.503603	5000.349107	7.374208	-0.036733	3.837682
182.779966	5008.355640	7.379213	-0.036789	3.840632
182.804078	5016.335902	7.384218	-0.036799	3.843564
182.968638	5024.376502	7.389222	-0.036834	3.846519
183.140260	5032.431481	7.394227	-0.036871	3.849477
183.413447	5040.435950	7.399232	-0.036927	3.852416
183.596054	5048.522469	7.404237	-0.036966	3.855382
183.854432	5056.465167	7.409242	-0.037019	3.858294
183.978861	5064.493114	7.414246	-0.037048	3.861232
184.225288	5072.523096	7.419251	-0.037098	3.864171
184.290442	5080.570086	7.424256	-0.037116	3.867110
184.573377	5088.641312	7.429261	-0.037173	3.870060
184.807431	5096.804587	7.434266	-0.037222	3.873041
184.929080	5104.859457	7.439270	-0.037250	3.875978
185.096584	5112.777303	7.444275	-0.037286	3.878863
185.107815	5120.762766	7.449280	-0.037293	3.881768
185.188021	5128.708418	7.454285	-0.037313	3.884657
185.334319	5136.727014	7.459290	-0.037345	3.887572
185.591817	5144.752666	7.464294	-0.037398	3.890490
185.900923	5152.786893	7.469299	-0.037461	3.893409
185.923615	5160.820867	7.474304	-0.037470	3.896321
186.003007	5168.812169	7.479309	-0.037490	3.899216
186.231212	5176.838766	7.484314	-0.037537	3.902124
186.524082	5184.825751	7.489318	-0.037597	3.905017
186.637570	5192.880858	7.494323	-0.037623	3.907929
186.897812	5200.871267	7.499328	-0.037677	3.910819
186.953964	5208.952701	7.504333	-0.037692	3.913735
186.999992	5216.940208	7.509338	-0.037706	3.916615
187.222548	5224.922839	7.514342	-0.037752	3.919495
187.437285	5232.972580	7.519347	-0.037797	3.922396
187.641069	5240.925602	7.524352	-0.037840	3.925260
187.908202	5248.982988	7.529357	-0.037895	3.928161
187.981000	5257.012779	7.534362	-0.037913	3.931046
188.177239	5265.063187	7.539366	-0.037955	3.933938
188.374167	5273.103899	7.544371	-0.037997	3.936825
188.536636	5281.052963	7.549376	-0.038032	3.939676
188.605141	5289.111964	7.554381	-0.038050	3.942563
188.659991	5297.090299	7.559386	-0.038065	3.945419
188.942974	5305.113856	7.564390	-0.038123	3.948293
189.187787	5313.163618	7.569395	-0.038173	3.951173
189.189139	5321.224277	7.574400	-0.038179	3.954051
189.678239	5329.210148	7.579405	-0.038275	3.956909
189.921239	5337.164015	7.584410	-0.038325	3.959748
189.942680	5345.173862	7.589414	-0.038334	3.962602
190.190533	5353.211936	7.594419	-0.038385	3.965468
190.168226	5361.243430	7.599424	-0.038386	3.968325
190.572871	5369.271742	7.604429	-0.038466	3.971185
190.665549	5377.321737	7.609434	-0.038489	3.974046
190.695186	5385.351530	7.614438	-0.038499	3.976897
191.069224	5393.340921	7.619443	-0.038574	3.979737
191.084063	5401.331910	7.624448	-0.038582	3.982570
191.192570	5409.369190	7.629453	-0.038607	3.985418
191.257462	5417.412539	7.634458	-0.038624	3.988266
191.529934	5425.437914	7.639462	-0.038680	3.991109
191.800876	5433.492178	7.644467	-0.038735	3.993960
191.804837	5441.518617	7.649472	-0.038741	3.996795
192.053897	5449.507679	7.654477	-0.038793	3.999618
191.936738	5457.528057	7.659482	-0.038776	4.002445
192.335889	5465.490734	7.664486	-0.038855	4.005258
192.591580	5473.568540	7.669491	-0.038908	4.008106
192.659415	5481.590560	7.674496	-0.038925	4.010931
192.907771	5489.638594	7.679501	-0.038977	4.013765
193.243792	5497.654743	7.684506	-0.039044	4.016587
193.289245	5505.653130	7.689510	-0.039058	4.019396
193.387098	5513.718008	7.694515	-0.039081	4.022228
193.462769	5521.660458	7.699520	-0.039100	4.025015
193.649242	5529.757771	7.704525	-0.039140	4.027855
193.852895	5537.737059	7.709530	-0.039183	4.030652
194.063078	5545.856463	7.714534	-0.039227	4.033497
194.278846	5553.866241	7.719539	-0.039272	4.036301
194.444391	5561.812352	7.724544	-0.039308	4.039080
194.720784	5569.829016	7.729549	-0.039365	4.041884
194.709547	5577.796526	7.734554	-0.039367	4.044664
194.937886	5585.818447	7.739558	-0.039415	4.047465
195.143454	5593.834443	7.744563	-0.039458	4.050261
195.126593	5601.874407	7.749568	-0.039460	4.053060
195.413884	5609.894615	7.754573	-0.039519	4.055856
195.452789	5617.903904	7.759578	-0.039531	4.058641
195.758462	5625.915729	7.764582	-0.039593	4.061430
195.896546	5633.919437	7.769587	-0.039624	4.064211
195.851966	5641.956006	7.774592	-0.039620	4.067000
196.091117	5649.976555	7.779597	-0.039670	4.069784
196.337059	5658.010538	7.784602	-0.039721	4.072572
196.477349	5666.016543	7.789606	-0.039752	4.075347
196.559413	5674.041249	7.794611	-0.039772	4.078125
196.673899	5682.009662	7.799616	-0.039799	4.080882
197.117738	5690.056202	7.804621	-0.039886	4.083669
197.124209	5698.084231	7.809626	-0.039893	4.086442
197.162169	5706.063991	7.814630	-0.039905	4.089196
197.358774	5714.174205	7.819635	-0.039946	4.091996
197.430671	5722.147249	7.824640	-0.039965	4.094745
197.797512	5730.209395	7.829645	-0.040038	4.097527
198.213276	5738.170933	7.834650	-0.040120	4.100273
198.169540	5746.172071	7.839654	-0.040117	4.103024
198.232170	5754.199014	7.844659	-0.040134	4.105784
198.415402	5762.226782	7.849664	-0.040173	4.108544
198.597686	5770.304649	7.854669	-0.040212	4.111319
198.836503	5778.353142	7.859674	-0.040262	4.114083
199.145859	5786.368056	7.864678	-0.040324	4.116834
199.261213	5794.309121	7.869683	-0.040351	4.119556
199.326279	5802.344031	7.874688	-0.040368	4.122307
199.478626	5810.344594	7.879693	-0.040401	4.125046
199.856973	5818.367793	7.884698	-0.040477	4.127794
200.010324	5826.380983	7.889702	-0.040510	4.130534
200.241355	5834.449785	7.894707	-0.040558	4.133291
200.079580	5842.477913	7.899712	-0.040533	4.136028
200.531400	5850.467180	7.904717	-0.040622	4.138758
200.815586	5858.491760	7.909722	-0.040680	4.141496
200.865628	5866.447583	7.914726	-0.040695	4.144205
201.143870	5874.527196	7.919731	-0.040752	4.146958
201.095254	5882.530159	7.924736	-0.040748	4.149679
201.181616	5890.607145	7.929741	-0.040769	4.152424
201.446249	5898.611566	7.934746	-0.040823	4.155146
201.461305	5906.604248	7.939750	-0.040831	4.157859
201.719924	5914.627825	7.944755	-0.040884	4.160583
201.772889	5922.613156	7.949760	-0.040899	4.163290
202.163518	5930.664106	7.954765	-0.040977	4.166021
202.101696	5938.660206	7.959770	-0.040970	4.168727
202.203151	5946.676284	7.964774	-0.040994	4.171440
202.580845	5954.729011	7.969779	-0.041069	4.174166
202.538300	5962.771599	7.974784	-0.041067	4.176883
202.833249	5970.725891	7.979789	-0.041127	4.179571
203.111723	5978.772989	7.984794	-0.041183	4.182289
203.289159	5986.750020	7.989798	-0.041221	4.184981
203.393520	5994.793039	7.994803	-0.041246	4.187692
203.489517	6002.834171	7.999808	-0.041269	4.190401
203.883098	6010.928517	8.004813	-0.041347	4.193129
203.723761	6018.955907	8.009818	-0.041323	4.195826
203.783824	6026.885713	8.014822	-0.041339	4.198492
204.056733	6034.905921	8.019827	-0.041395	4.201189
204.241674	6042.875542	8.024832	-0.041434	4.203865
204.402215	6050.896711	8.029837	-0.041469	4.206557
204.892784	6058.867200	8.034842	-0.041565	4.209234
204.917537	6066.941235	8.039846	-0.041575	4.211939
205.096282	6075.008298	8.044851	-0.041613	4.214642
205.140659	6082.992292	8.049856	-0.041627	4.217313
205.653100	6090.963484	8.054861	-0.041727	4.219983
205.724867	6099.029824	8.059866	-0.041745	4.222679
205.427852	6107.006676	8.064870	-0.041695	4.225340
205.770983	6115.061173	8.069875	-0.041764	4.228031
206.022914	6123.049655	8.074880	-0.041816	4.230697
206.229940	6131.090518	8.079885	-0.041860	4.233379
206.332135	6139.127428	8.084890	-0.041884	4.236057
206.500653	6147.077483	8.089894	-0.041920	4.238705
206.745787	6155.147745	8.094899	-0.041971	4.241391
206.749364	6163.119256	8.099904	-0.041976	4.244041
206.944001	6171.215379	8.104909	-0.042018	4.246733
207.008048	6179.155781	8.109914	-0.042035	4.249370
207.195933	6187.227581	8.114918	-0.042075	4.252050
207.522889	6195.244195	8.119923	-0.042141	4.254711
207.546630	6203.255462	8.124928	-0.042150	4.257366
207.610825	6211.254610	8.129933	-0.042167	4.260015
207.858326	6219.273614	8.134938	-0.042218	4.262672
207.983864	6227.310454	8.139942	-0.042246	4.265331
208.109462	6235.359925	8.144947	-0.042275	4.267993
208.355988	6243.324294	8.149952	-0.042326	4.270626
208.635936	6251.425242	8.154957	-0.042383	4.273303
208.778749	6259.436532	8.159962	-0.042415	4.275947
208.773730	6267.390382	8.164966	-0.042419	4.278570
208.779123	6275.437937	8.169971	-0.042425	4.281221
209.086423	6283.419233	8.174976	-0.042487	4.283852
209.213169	6291.466135	8.179981	-0.042516	4.286502
209.285318	6299.483366	8.184986	-0.042534	4.289139
209.377184	6307.514577	8.189990	-0.042556	4.291780
209.637682	6315.555155	8.194995	-0.042610	4.294423
209.490982	6323.557542	8.200000	-0.042587	4.297049
209.695856	6331.520975	8.205005	-0.042631	4.299663
209.943922	6339.584495	8.210010	-0.042682	4.302309
209.940093	6347.572409	8.215014	-0.042686	4.304927
210.385158	6355.624113	8.220019	-0.042774	4.307567
210.405549	6363.642311	8.225024	-0.042783	4.310191
210.864081	6371.671378	8.230029	-0.042873	4.312821
210.794936	6379.693913	8.235034	-0.042865	4.315443
210.811242	6387.659111	8.240038	-0.042873	4.318045
210.939341	6395.708836	8.245043	-0.042902	4.320674
211.010324	6403.695904	8.250048	-0.042921	4.323281
211.355177	6411.711365	8.255053	-0.042990	4.325897
211.619421	6419.722121	8.260058	-0.043044	4.328509
211.486219	6427.696738	8.265062	-0.043024	4.331106
211.608504	6435.809627	8.270067	-0.043052	4.333747
211.909402	6443.771003	8.275072	-0.043113	4.336339
212.213537	6451.784270	8.280077	-0.043175	4.338946
212.238068	6459.850733	8.285082	-0.043184	4.341567
212.426854	6467.818596	8.290086	-0.043225	4.344156
212.853031	6475.873909	8.295091	-0.043309	4.346773
212.813187	6483.844718	8.300096	-0.043307	4.349357
213.200074	6491.950258	8.305101	-0.043384	4.351987
213.433539	6500.031199	8.310106	-0.043432	4.354606
213.455502	6507.959290	8.315110	-0.043441	4.357173
213.619762	6515.947153	8.320115	-0.043477	4.359758
213.721455	6523.936235	8.325120	-0.043501	4.362342
213.905716	6531.920757	8.330125	-0.043540	4.364923
214.047209	6540.017285	8.335130	-0.043572	4.367539
214.216916	6547.968213	8.340134	-0.043608	4.370106
214.468824	6556.026895	8.345139	-0.043660	4.372707
214.536466	6564.032908	8.350144	-0.043678	4.375288
214.643462	6572.056524	8.355149	-0.043703	4.377874
214.917620	6580.056645	8.360154	-0.043759	4.380451
214.856958	6588.065739	8.365158	-0.043752	4.383028
215.071994	6596.108559	8.370163	-0.043798	4.385616
215.153293	6604.123623	8.375168	-0.043818	4.388192
215.381074	6612.136971	8.380173	-0.043865	4.390768
215.426719	6620.196229	8.385178	-0.043879	4.393355
215.530898	6628.167762	8.390182	-0.043903	4.395913
215.672754	6636.197885	8.395187	-0.043935	4.398489
215.595426	6644.185791	8.400192	-0.043925	4.401049
215.955659	6652.189577	8.405197	-0.043997	4.403614
216.134581	6660.209940	8.410202	-0.044036	4.406182
216.168652	6668.204220	8.415206	-0.044047	4.408740
216.370751	6676.271773	8.420211	-0.044090	4.411320
216.378606	6684.297370	8.425216	-0.044096	4.413884
216.569998	6692.336508	8.430221	-0.044137	4.416452
216.571264	6700.320723	8.435226	-0.044142	4.419001
216.717645	6708.364125	8.440230	-0.044174	4.421567
217.084189	6716.413849	8.445235	-0.044248	4.424135
217.115723	6724.410649	8.450240	-0.044259	4.426683
217.383931	6732.392911	8.455245	-0.044313	4.429226
217.462954	6740.425792	8.460250	-0.044333	4.431782
217.716163	6748.475591	8.465254	-0.044385	4.434343
217.941725	6756.504998	8.470259	-0.044432	4.436897
218.096463	6764.462447	8.475264	-0.044466	4.439425
218.123260	6772.499043	8.480269	-0.044476	4.441977
218.263642	6780.501344	8.485274	-0.044507	4.444516
218.354283	6788.515840	8.490278	-0.044529	4.447058
218.577461	6796.530271	8.495283	-0.044576	4.449599
218.691203	6804.576427	8.500288	-0.044602	4.452149
218.686666	6812.583373	8.505293	-0.044606	4.454683
218.897517	6820.616863	8.510298	-0.044651	4.457226
218.925709	6828.584201	8.515302	-0.044661	4.459745
219.146704	6836.615976	8.520307	-0.044707	4.462284
219.252455	6844.587552	8.525312	-0.044732	4.464803
219.445288	6852.656637	8.530317	-0.044773	4.467351
219.633800	6860.665131	8.535322	-0.044813	4.469878
219.770461	6868.712503	8.540326	-0.044843	4.472416
220.004216	6876.751532	8.545331	-0.044892	4.474950
220.113016	6884.735112	8.550336	-0.044917	4.477465
220.105743	6892.692733	8.555341	-0.044921	4.479969
220.395422	6900.756892	8.560346	-0.044980	4.482507
220.548194	6908.729828	8.565351	-0.045013	4.485014
220.715549	6916.802550	8.570355	-0.045049	4.487552
220.823447	6924.796982	8.575360	-0.045075	4.490063
221.048102	6932.838570	8.580365	-0.045121	4.492588
221.079585	6940.898581	8.585370	-0.045132	4.495116
221.093017	6948.868694	8.590375	-0.045140	4.497615
221.445157	6956.872020	8.595379	-0.045210	4.500124
221.708156	6964.871788	8.600384	-0.045264	4.502630
221.717885	6972.859404	8.605389	-0.045271	4.505130
222.076081	6980.936308	8.610394	-0.045343	4.507657
222.223889	6988.912792	8.615399	-0.045376	4.510152
222.288236	6997.014376	8.620403	-0.045393	4.512683
222.265210	7005.019247	8.625408	-0.045393	4.515183
222.508745	7012.988437	8.630413	-0.045444	4.517671
222.442797	7021.003538	8.635418	-0.045436	4.520171
222.582127	7028.954413	8.640423	-0.045467	4.522650
222.895679	7036.934501	8.645427	-0.045531	4.525138
223.013487	7045.001721	8.650432	-0.045558	4.527650
223.067532	7053.007696	8.655437	-0.045573	4.530142
223.077635	7061.105740	8.660442	-0.045580	4.532661
223.340949	7069.037908	8.665447	-0.045634	4.535128
223.605887	7077.127254	8.670451	-0.045688	4.537642
223.896816	7085.059144	8.675456	-0.045747	4.540106
224.143225	7093.105393	8.680461	-0.045798	4.542604
224.252248	7101.092535	8.685466	-0.045824	4.545082
224.091053	7109.157091	8.690471	-0.045799	4.547582
224.431133	7117.147773	8.695475	-0.045867	4.550059
224.405918	7125.194234	8.700480	-0.045867	4.552551
224.475455	7133.242616	8.705485	-0.045885	4.555042
224.500631	7141.263347	8.710490	-0.045895	4.557523
224.700259	7149.209902	8.715495	-0.045937	4.559981
224.991280	7157.279675	8.720499	-0.045996	4.562475
224.894489	7165.206969	8.725504	-0.045983	4.564923
225.297794	7173.247782	8.730509	-0.046063	4.567406
225.298077	7181.321987	8.735514	-0.046069	4.569897
225.456993	7189.321042	8.740519	-0.046103	4.572363
225.720222	7197.359599	8.745523	-0.046157	4.574841
225.622541	7205.391609	8.750528	-0.046144	4.577315
225.756076	7213.344059	8.755533	-0.046174	4.579763
226.008603	7221.409090	8.760538	-0.046226	4.582245
226.198982	7229.355885	8.765543	-0.046266	4.584689
226.368898	7237.438122	8.770547	-0.046303	4.587173
226.299887	7245.467398	8.775552	-0.046295	4.589639
226.619518	7253.492049	8.780557	-0.046360	4.592103
226.688142	7261.531779	8.785562	-0.046378	4.594570
226.570082	7269.547657	8.790567	-0.046361	4.597029
226.748921	7277.475667	8.795571	-0.046399	4.599459
227.109398	7285.537178	8.800576	-0.046471	4.601928
227.247171	7293.468774	8.805581	-0.046502	4.604357
227.324738	7301.588351	8.810586	-0.046521	4.606842
227.454831	7309.498925	8.815591	-0.046551	4.609261
227.635303	7317.619021	8.820595	-0.046589	4.611744
227.808525	7325.602521	8.825600	-0.046626	4.614183
227.683387	7333.649658	8.830605	-0.046608	4.616640
227.994552	7341.653001	8.835610	-0.046671	4.619083
228.146955	7349.641208	8.840615	-0.046705	4.621520
228.228497	7357.658245	8.845619	-0.046725	4.623964
228.466164	7365.649952	8.850624	-0.046774	4.626399
228.368761	7373.684634	8.855629	-0.046761	4.628846
228.562944	7381.719750	8.860634	-0.046802	4.631292
228.742960	7389.723253	8.865639	-0.046841	4.633727
229.030962	7397.765094	8.870643	-0.046899	4.636172
228.958548	7405.733630	8.875648	-0.046891	4.638594
229.184045	7413.759298	8.880653	-0.046938	4.641031
229.507689	7421.775082	8.885658	-0.047003	4.643465
229.215986	7429.776319	8.890663	-0.046954	4.645893
229.470760	7437.835491	8.895667	-0.047006	4.648336
229.671998	7445.830872	8.900672	-0.047049	4.650760
230.041338	7453.852632	8.905677	-0.047123	4.653190
230.019123	7461.895080	8.910682	-0.047124	4.655625
230.108365	7469.867802	8.915687	-0.047145	4.658037
230.322445	7477.884359	8.920691	-0.047190	4.660462
230.279504	7485.905283	8.925696	-0.047187	4.662887
230.384426	7493.934038	8.930701	-0.047212	4.665313
230.719479	7501.976215	8.935706	-0.047279	4.667741
230.611102	7509.897736	8.940711	-0.047264	4.670132
230.705365	7518.037411	8.945715	-0.047287	4.672588
230.971094	7526.087951	8.950720	-0.047341	4.675015
231.204763	7534.061807	8.955725	-0.047390	4.677417
231.414402	7542.014857	8.960730	-0.047434	4.679812
231.439691	7550.040615	8.965735	-0.047443	4.682229
231.631823	7557.995669	8.970739	-0.047484	4.684622
231.494601	7566.067263	8.975744	-0.047464	4.687050
231.671915	7574.056498	8.980749	-0.047502	4.689451
232.128119	7582.140957	8.985754	-0.047592	4.691879
232.119450	7590.078210	8.990759	-0.047595	4.694262
232.004893	7598.118720	8.995763	-0.047579	4.696675
232.233628	7606.117684	9.000768	-0.047626	4.699074
232.378530	7614.130682	9.005773	-0.047658	4.701476
232.598459	7622.130645	9.010778	-0.047704	4.703873
232.799286	7630.146113	9.015783	-0.047747	4.706273
233.099275	7638.198824	9.020787	-0.047808	4.708683
233.223875	7646.166790	9.025792	-0.047836	4.711067
233.381695	7654.246665	9.030797	-0.047870	4.713483
233.685452	7662.293248	9.035802	-0.047932	4.715887
233.557349	7670.199442	9.040807	-0.047913	4.718249
233.619514	7678.265925	9.045811	-0.047930	4.720657
233.715460	7686.299173	9.050816	-0.047953	4.723054
233.816655	7694.262258	9.055821	-0.047976	4.725429
233.908883	7702.369680	9.060826	-0.047999	4.727846
233.761704	7710.321919	9.065831	-0.047976	4.730216
234.281462	7718.354525	9.070835	-0.048078	4.732607
234.385633	7726.403208	9.075840	-0.048102	4.735002
234.353708	7734.398021	9.080845	-0.048102	4.737381
234.679268	7742.412968	9.085850	-0.048167	4.739763
234.842753	7750.446214	9.090855	-0.048203	4.742150
234.956410	7758.389509	9.095859	-0.048229	4.744510
234.913094	7766.487676	9.100864	-0.048226	4.746914
235.112658	7774.459931	9.105869	-0.048268	4.749280
235.245573	7782.499746	9.110874	-0.048298	4.751664
235.280357	7790.529936	9.115879	-0.048309	4.754044
235.394686	7798.550309	9.120883	-0.048336	4.756420
235.742319	7806.516248	9.125888	-0.048405	4.758779
235.581183	7814.541566	9.130893	-0.048380	4.761155
235.768709	7822.547507	9.135898	-0.048420	4.763523
235.800825	7830.531360	9.140903	-0.048431	4.765884
235.871447	7838.576714	9.145907	-0.048449	4.768261
236.274324	7846.604859	9.150912	-0.048530	4.770632
236.533885	7854.636416	9.155917	-0.048583	4.773002
236.670554	7862.651457	9.160922	-0.048613	4.775367
236.658266	7870.619904	9.165927	-0.048616	4.777718
236.733485	7878.616729	9.170931	-0.048635	4.780075
236.801681	7886.719177	9.175936	-0.048653	4.782462
236.723522	7894.614860	9.180941	-0.048643	4.784788
237.167963	7902.751723	9.185946	-0.048731	4.787182
237.139095	7910.681414	9.190951	-0.048731	4.789515
237.347454	7918.738304	9.195955	-0.048775	4.791884
237.236782	7926.784076	9.200960	-0.048759	4.794249
237.488116	7934.808217	9.205965	-0.048811	4.796606
237.839182	7942.766628	9.210970	-0.048881	4.798942
237.770430	7950.744079	9.215975	-0.048873	4.801283
237.975230	7958.799788	9.220979	-0.048917	4.803646
238.161393	7966.806016	9.225984	-0.048956	4.805993
238.214697	7974.784344	9.230989	-0.048971	4.808331
238.419885	7982.833992	9.235994	-0.049014	4.810688
238.484152	7990.314844	9.240999	-0.049031	4.812878
238.861815	7995.060049	9.246003	-0.049104	4.814265

238.646099	7997.601154	9.251008	-0.049066	4.815010
238.797376	7998.987510	9.256013	-0.049094	4.815414
239.138157	7999.487041	9.261018	-0.049158	4.815559
239.152761	8000.378331	9.266023	-0.049161	4.815820
239.163302	8000.394492	9.271027	-0.049163	4.815824
239.297241	8000.387028	9.276032	-0.049188	4.815822
239.326239	8000.384276	9.281037	-0.049193	4.815821
239.597008	8000.422772	9.286042	-0.049243	4.815831
239.503019	8000.371082	9.291047	-0.049225	4.815816
239.501970	8000.397728	9.296051	-0.049225	4.815824
239.377656	8000.379700	9.301056	-0.049202	4.815819
239.666370	8000.381133	9.306061	-0.049255	4.815818
239.564601	8000.396551	9.311066	-0.049236	4.815823
239.472540	8000.370506	9.316071	-0.049219	4.815816
239.712187	8000.401030	9.321075	-0.049263	4.815824
239.895522	8000.412504	9.326080	-0.049297	4.815826
239.637893	8000.384858	9.331085	-0.049249	4.815819
239.778363	8000.420187	9.336090	-0.049275	4.815829
239.725106	8000.362750	9.341095	-0.049265	4.815813
239.759924	8000.433729	9.346099	-0.049271	4.815833
239.798323	8000.394845	9.351104	-0.049278	4.815822
239.789257	8000.391480	9.356109	-0.049276	4.815821
239.790244	8000.420293	9.361114	-0.049276	4.815829
239.715154	8000.410528	9.366119	-0.049262	4.815827
239.912190	8000.429694	9.371123	-0.049298	4.815831
240.069085	8000.375644	9.376128	-0.049327	4.815815
239.926958	8000.402151	9.381133	-0.049301	4.815823
239.934583	8000.412929	9.386138	-0.049302	4.815826
239.984150	8000.372089	9.391143	-0.049311	4.815814
240.276647	8000.422676	9.396147	-0.049365	4.815828
240.334387	8000.381968	9.401152	-0.049376	4.815815
240.455022	8000.388165	9.406157	-0.049398	4.815817
240.423228	8000.418584	9.411162	-0.049392	4.815826
240.316620	8000.386967	9.416167	-0.049372	4.815817
240.175915	8000.411362	9.421171	-0.049346	4.815825
240.136113	8000.379755	9.426176	-0.049338	4.815816
240.244211	8000.397488	9.431181	-0.049358	4.815820
240.236473	8000.411220	9.436186	-0.049356	4.815824
240.228148	8000.398262	9.441191	-0.049354	4.815821
240.347852	8000.423653	9.446195	-0.049377	4.815828
240.503837	8000.382394	9.451200	-0.049405	4.815815
240.405013	8000.417069	9.456205	-0.049387	4.815825
240.587409	8000.419992	9.461210	-0.049421	4.815825
240.535867	8000.389262	9.466215	-0.049411	4.815817
240.433551	8000.418545	9.471219	-0.049392	4.815826
240.659479	8000.439246	9.476224	-0.049433	4.815831
240.562313	8000.397108	9.481229	-0.049415	4.815819
240.628196	8000.432304	9.486234	-0.049427	4.815829
240.453027	8000.423060	9.491239	-0.049394	4.815827
240.526291	8000.415686	9.496243	-0.049408	4.815824
240.279024	8000.398877	9.501248	-0.049362	4.815821
240.344747	8000.420196	9.506253	-0.049374	4.815827
240.659759	8000.445534	9.511258	-0.049432	4.815833
240.349866	8000.379690	9.516263	-0.049374	4.815815
240.365007	8000.399127	9.521267	-0.049377	4.815820
240.731959	8000.397554	9.526272	-0.049445	4.815818
240.468802	8000.384757	9.531277	-0.049396	4.815816
240.633126	8000.438615	9.536282	-0.049426	4.815831
240.652162	8000.393015	9.541287	-0.049429	4.815817
240.686590	8000.388217	9.546291	-0.049436	4.815816
240.464028	8000.394217	9.551296	-0.049394	4.815818
240.592731	8000.393073	9.556301	-0.049418	4.815818
240.490891	8000.398885	9.561306	-0.049399	4.815820
240.467675	8000.388888	9.566311	-0.049394	4.815817
240.501628	8000.415032	9.571315	-0.049400	4.815824
240.722634	8000.397233	9.576320	-0.049441	4.815818
240.709527	8000.410878	9.581325	-0.049439	4.815822
240.477305	8000.384706	9.586330	-0.049395	4.815816
240.490547	8000.384903	9.591335	-0.049397	4.815816
240.703429	8000.397922	9.596339	-0.049437	4.815818
240.721263	8000.403528	9.601344	-0.049440	4.815820
240.546342	8000.406028	9.606349	-0.049407	4.815822
240.939008	8000.415542	9.611354	-0.049480	4.815823
240.672360	8000.374941	9.616359	-0.049430	4.815812
240.582148	8000.419360	9.621363	-0.049413	4.815825
240.565529	8000.395596	9.626368	-0.049410	4.815818
240.640993	8000.403199	9.631373	-0.049424	4.815820
240.638578	8000.423420	9.636378	-0.049423	4.815826
240.615059	8000.387806	9.641383	-0.049419	4.815816
240.816874	8000.411319	9.646387	-0.049456	4.815822
240.922865	8000.402338	9.651392	-0.049476	4.815819
240.919611	8000.392664	9.656397	-0.049475	4.815816
240.909912	8000.412768	9.661402	-0.049473	4.815822
240.871315	8000.388649	9.666407	-0.049465	4.815815
240.840974	8000.415891	9.671411	-0.049460	4.815823
241.111118	8000.393548	9.676416	-0.049510	4.815815
241.000228	8000.394945	9.681421	-0.049489	4.815816
240.848015	8000.376466	9.686426	-0.049460	4.815812
240.802629	8000.383188	9.691431	-0.049452	4.815814
241.012311	8000.412164	9.696435	-0.049490	4.815821
240.918296	8000.420237	9.701440	-0.049473	4.815824
240.807422	8000.387483	9.706445	-0.049452	4.815815
240.913173	8000.439330	9.711450	-0.049471	4.815830
241.067763	8000.400183	9.716455	-0.049500	4.815818
240.964403	8000.428382	9.721459	-0.049481	4.815826
241.046619	8000.423287	9.726464	-0.049496	4.815824
241.100695	8000.396394	9.731469	-0.049505	4.815816
240.923583	8000.410597	9.736474	-0.049472	4.815821
240.880233	8000.352251	9.741479	-0.049464	4.815804
241.043086	8000.384741	9.746483	-0.049494	4.815813
241.110774	8000.443446	9.751488	-0.049507	4.815830
240.959642	8000.385496	9.756493	-0.049478	4.815814
241.039002	8000.410238	9.761498	-0.049493	4.815821
241.027649	8000.423912	9.766503	-0.049491	4.815825
241.092859	8000.419610	9.771507	-0.049502	4.815823
241.170217	8000.425109	9.776512	-0.049517	4.815824
241.087212	8000.408812	9.781517	-0.049501	4.815820
241.142520	8000.464115	9.786522	-0.049511	4.815836
241.086243	8000.401292	9.791527	-0.049500	4.815818
241.296213	8000.422803	9.796531	-0.049539	4.815823
241.180530	8000.446534	9.801536	-0.049518	4.815831
241.194259	8000.412587	9.806541	-0.049520	4.815821
241.172611	8000.426095	9.811546	-0.049516	4.815825
241.109579	8000.384507	9.816551	-0.049504	4.815813
241.150999	8000.418241	9.821555	-0.049511	4.815823
241.054738	8000.409202	9.826560	-0.049493	4.815820
241.241049	8000.401516	9.831565	-0.049528	4.815817
241.158112	8000.425775	9.836570	-0.049512	4.815825
241.249511	8000.416560	9.841575	-0.049529	4.815822
241.158048	8000.443883	9.846579	-0.049512	4.815830
241.313199	8000.431426	9.851584	-0.049540	4.815826
241.110864	8000.399332	9.856589	-0.049502	4.815817
241.368842	8000.432289	9.861594	-0.049550	4.815826
241.257589	8000.410201	9.866599	-0.049529	4.815820
241.295173	8000.424664	9.871603	-0.049536	4.815824
241.260546	8000.403811	9.876608	-0.049530	4.815818
241.391629	8000.388832	9.881613	-0.049554	4.815813
241.280838	8000.422247	9.886618	-0.049533	4.815823
241.135136	8000.399603	9.891623	-0.049506	4.815817
241.311758	8000.413106	9.896627	-0.049538	4.815820
241.457276	8000.413301	9.901632	-0.049565	4.815820
241.443681	8000.401325	9.906637	-0.049562	4.815816
241.415552	8000.417930	9.911642	-0.049557	4.815821
241.597319	8000.405903	9.916647	-0.049591	4.815817
241.522012	8000.435621	9.921651	-0.049576	4.815826
241.659099	8000.419672	9.926656	-0.049602	4.815821
241.465551	8000.421870	9.931661	-0.049566	4.815822
241.555790	8000.437182	9.936666	-0.049582	4.815826
241.365580	8000.406349	9.941671	-0.049547	4.815818
241.648714	8000.422637	9.946675	-0.049599	4.815822
241.590320	8000.440889	9.951680	-0.049588	4.815827
241.318207	8000.411938	9.956685	-0.049537	4.815820
241.477438	8000.431564	9.961690	-0.049567	4.815825
241.574581	8000.412836	9.966695	-0.049584	4.815819
241.576945	8000.422462	9.971699	-0.049585	4.815822
241.595805	8000.434488	9.976704	-0.049588	4.815825
241.593251	8000.434430	9.981709	-0.049587	4.815825
241.522361	8000.482363	9.986714	-0.049574	4.815840
241.302440	8000.467060	9.991719	-0.049533	4.815836
241.371695	8000.482034	9.996723	-0.049546	4.815840
241.551636	8000.452901	10.001728	-0.049579	4.815831
241.490423	8000.430552	10.006733	-0.049567	4.815825
241.286629	8000.456064	10.011738	-0.049529	4.815833
241.324900	8000.416109	10.016743	-0.049536	4.815821
241.490916	8000.428374	10.021747	-0.049567	4.815824
241.452809	8000.436280	10.026752	-0.049559	4.815827
241.508284	8000.421149	10.031757	-0.049570	4.815822
241.465125	8000.457790	10.036762	-0.049561	4.815833
241.447564	8000.426539	10.041767	-0.049558	4.815824
241.417634	8000.403628	10.046771	-0.049552	4.815817
241.578376	8000.410471	10.051776	-0.049582	4.815818
241.571765	8000.401810	10.056781	-0.049580	4.815816
241.578803	8000.423251	10.061786	-0.049581	4.815822
241.620821	8000.405768	10.066791	-0.049589	4.815817
241.795044	8000.438444	10.071795	-0.049621	4.815826
241.665293	8000.461948	10.076800	-0.049597	4.815833
241.528592	8000.390356	10.081805	-0.049571	4.815813
241.742233	8000.418330	10.086810	-0.049611	4.815820
241.421911	8000.375795	10.091815	-0.049551	4.815809
241.529054	8000.426598	10.096819	-0.049571	4.815823
241.767231	8000.435758	10.101824	-0.049615	4.815825
241.759531	8000.416406	10.106829	-0.049613	4.815819
241.612771	8000.419359	10.111834	-0.049586	4.815821
241.644119	8000.403838	10.116839	-0.049591	4.815816
241.788454	8000.427494	10.121843	-0.049618	4.815823
241.841790	8000.432606	10.126848	-0.049628	4.815824
241.548360	8000.408646	10.131853	-0.049573	4.815818
241.817921	8000.440725	10.136858	-0.049623	4.815826
241.589782	8000.423154	10.141863	-0.049580	4.815822
241.565615	8000.415277	10.146867	-0.049576	4.815820
241.658096	8000.418885	10.151872	-0.049593	4.815821
241.660560	8000.407168	10.156877	-0.049593	4.815817
241.710606	8000.446379	10.161882	-0.049602	4.815828
241.648563	8000.436824	10.166887	-0.049590	4.815826
241.685558	8000.432067	10.171891	-0.049597	4.815824
241.618961	8000.451253	10.176896	-0.049584	4.815830
241.628281	8000.411899	10.181901	-0.049586	4.815819
241.730541	8000.443413	10.186906	-0.049605	4.815828
241.868095	8000.413597	10.191911	-0.049630	4.815818
241.634174	8000.431153	10.196915	-0.049586	4.815824
241.856505	8000.446461	10.201920	-0.049628	4.815828
241.709026	8000.422720	10.206925	-0.049600	4.815822
241.835649	8000.469570	10.211930	-0.049623	4.815835
241.753351	8000.438342	10.216935	-0.049608	4.815826
241.861842	8000.433671	10.221939	-0.049628	4.815824
241.785667	8000.456972	10.226944	-0.049614	4.815831
241.689093	8000.425515	10.231949	-0.049595	4.815823
241.644474	8000.437585	10.236954	-0.049587	4.815826
241.526362	8000.406848	10.241959	-0.049565	4.815818
241.672946	8000.431607	10.246963	-0.049592	4.815824
241.743003	8000.434854	10.251968	-0.049605	4.815825
241.808036	8000.398532	10.256973	-0.049616	4.815814
241.870840	8000.445419	10.261978	-0.049628	4.815828
241.823283	8000.451039	10.266983	-0.049619	4.815829
241.824509	8000.448907	10.271987	-0.049619	4.815829
241.822168	8000.447785	10.276992	-0.049618	4.815828
241.541838	8000.416566	10.281997	-0.049566	4.815821
241.735932	8000.437822	10.287002	-0.049602	4.815826
241.808260	8000.413357	10.292007	-0.049615	4.815818
241.659378	8000.408805	10.297011	-0.049587	4.815818
241.858753	8000.470701	10.302016	-0.049624	4.815835
241.860465	8000.456838	10.307021	-0.049624	4.815831
241.888663	8000.450872	10.312026	-0.049629	4.815829
241.821963	8000.431636	10.317031	-0.049617	4.815824
241.958799	8000.427422	10.322035	-0.049642	4.815822
242.000997	8000.433422	10.327040	-0.049650	4.815823
241.954436	8000.431586	10.332045	-0.049641	4.815823
241.830706	8000.441314	10.337050	-0.049618	4.815827
241.850169	8000.430938	10.342055	-0.049621	4.815823
241.837091	8000.436046	10.347059	-0.049618	4.815825
241.956064	8000.452889	10.352064	-0.049640	4.815829
242.031902	8000.428481	10.357069	-0.049654	4.815822
241.863320	8000.446023	10.362074	-0.049623	4.815828
241.943200	8000.427016	10.367079	-0.049637	4.815822
242.027661	8000.424093	10.372083	-0.049653	4.815821
242.224940	8000.433661	10.377088	-0.049689	4.815823
241.875480	8000.422671	10.382093	-0.049624	4.815821
241.872016	8000.435405	10.387098	-0.049623	4.815825
241.860746	8000.380777	10.392103	-0.049621	4.815809
241.905893	8000.412438	10.397107	-0.049629	4.815818
241.981387	8000.433916	10.402112	-0.049643	4.815824
241.958167	8000.410045	10.407117	-0.049638	4.815817
242.035409	8000.448627	10.412122	-0.049653	4.815828
241.991946	8000.355059	10.417127	-0.049644	4.815801
242.042800	8000.410291	10.422131	-0.049654	4.815817
242.088422	8000.433422	10.427136	-0.049662	4.815823
241.943102	8000.421456	10.432141	-0.049635	4.815820
242.020303	8000.449365	10.437146	-0.049649	4.815828
241.951954	8000.452515	10.442151	-0.049636	4.815829
241.815260	8000.423612	10.447155	-0.049610	4.815822
241.830240	8000.466526	10.452160	-0.049613	4.815834
241.773424	8000.415432	10.457165	-0.049602	4.815819
241.875493	8000.434137	10.462170	-0.049621	4.815824
241.859268	8000.410379	10.467175	-0.049618	4.815818
241.849996	8000.428356	10.472179	-0.049616	4.815823
242.013482	8000.444849	10.477184	-0.049646	4.815827
241.857006	8000.416695	10.482189	-0.049617	4.815819
242.055603	8000.461503	10.487194	-0.049654	4.815832
241.938478	8000.417975	10.492199	-0.049631	4.815819
242.008516	8000.404145	10.497203	-0.049644	4.815815
242.014734	8000.450120	10.502208	-0.049645	4.815828
242.199263	8000.405053	10.507213	-0.049679	4.815814
242.108628	8000.458004	10.512218	-0.049662	4.815830
242.118524	8000.426129	10.517223	-0.049664	4.815821
242.017380	8000.427682	10.522227	-0.049645	4.815822
242.125991	8000.441157	10.527232	-0.049665	4.815825
242.100967	8000.401248	10.532237	-0.049660	4.815814
241.994988	8000.444346	10.537242	-0.049640	4.815827
241.919764	8000.405762	10.542247	-0.049626	4.815816
241.861332	8000.404802	10.547251	-0.049615	4.815816
241.949636	8000.448899	10.552256	-0.049631	4.815828
242.005800	8000.416703	10.557261	-0.049641	4.815819
242.033586	8000.445950	10.562266	-0.049646	4.815827
241.936244	8000.446497	10.567271	-0.049628	4.815828
241.817275	8000.436024	10.572275	-0.049606	4.815825
241.938805	8000.478522	10.577280	-0.049628	4.815837
241.887326	8000.452061	10.582285	-0.049618	4.815830
241.766519	8000.450095	10.587290	-0.049596	4.815830
242.028086	8000.453229	10.592295	-0.049644	4.815829
242.047746	8000.363881	10.597299	-0.049648	4.815803
241.985142	8000.469578	10.602304	-0.049636	4.815834
241.939325	8000.412258	10.607309	-0.049627	4.815818
241.931390	8000.452669	10.612314	-0.049625	4.815830
241.824718	8000.431721	10.617319	-0.049605	4.815824
241.928501	8000.424839	10.622323	-0.049624	4.815822
242.047583	8000.463029	10.627328	-0.049646	4.815832
241.877002	8000.430378	10.632333	-0.049614	4.815823
242.027901	8000.434929	10.637338	-0.049642	4.815824
242.061892	8000.427989	10.642343	-0.049649	4.815822
241.854198	8000.407547	10.647347	-0.049610	4.815817
241.936907	8000.470764	10.652352	-0.049625	4.815835
241.839165	8000.406203	10.657357	-0.049606	4.815817
241.868421	8000.434406	10.662362	-0.049612	4.815825
241.915971	8000.445828	10.667367	-0.049620	4.815828
241.862232	8000.421465	10.672371	-0.049610	4.815821
242.034942	8000.459452	10.677376	-0.049642	4.815831
241.913877	8000.419062	10.682381	-0.049619	4.815820
242.126650	8000.433149	10.687386	-0.049659	4.815823
242.122296	8000.430927	10.692391	-0.049658	4.815823
242.133454	8000.442830	10.697395	-0.049660	4.815826
242.133523	8000.456688	10.702400	-0.049660	4.815830
241.908352	8000.437030	10.707405	-0.049617	4.815825
242.143830	8000.446147	10.712410	-0.049661	4.815827
242.080690	8000.420565	10.717415	-0.049649	4.815820
242.198859	8000.442732	10.722419	-0.049671	4.815826
242.389582	8000.491683	10.727424	-0.049706	4.815839
242.276753	8000.448223	10.732429	-0.049685	4.815827
242.155726	8000.486809	10.737434	-0.049662	4.815839
242.203096	8000.497162	10.742439	-0.049671	4.815842
242.026539	8000.472952	10.747443	-0.049638	4.815835
242.150702	8000.451458	10.752448	-0.049661	4.815828
241.938173	8000.442676	10.757453	-0.049621	4.815827
242.072333	8000.409604	10.762458	-0.049646	4.815817
242.191729	8000.470211	10.767463	-0.049668	4.815834
242.007253	8000.448008	10.772467	-0.049633	4.815828
242.113872	8000.483863	10.777472	-0.049653	4.815838
242.010457	8000.475774	10.782477	-0.049633	4.815836
242.049615	8000.481725	10.787482	-0.049641	4.815838
242.206491	8000.462893	10.792487	-0.049670	4.815832
242.044462	8000.427178	10.797491	-0.049639	4.815822
242.046227	8000.465610	10.802496	-0.049639	4.815833
241.913272	8000.453843	10.807501	-0.049614	4.815830
242.138829	8000.483078	10.812506	-0.049656	4.815838
242.089607	8000.477998	10.817511	-0.049647	4.815837
241.971843	8000.422719	10.822515	-0.049625	4.815821
242.173722	8000.450505	10.827520	-0.049662	4.815828
242.166280	8000.432225	10.832525	-0.049660	4.815823
242.208800	8000.451036	10.837530	-0.049668	4.815828
242.245309	8000.465483	10.842535	-0.049675	4.815832
242.081188	8000.436137	10.847539	-0.049644	4.815824
242.164986	8000.480162	10.852544	-0.049659	4.815837
242.156886	8000.455467	10.857549	-0.049658	4.815830
242.253763	8000.392977	10.862554	-0.049676	4.815811
242.329882	8000.452887	10.867559	-0.049690	4.815828
242.290675	8000.445834	10.872563	-0.049682	4.815826
242.270872	8000.448699	10.877568	-0.049678	4.815827
242.312714	8000.421608	10.882573	-0.049686	4.815819
242.349265	8000.469140	10.887578	-0.049692	4.815833
242.361306	8000.453308	10.892583	-0.049694	4.815828
242.358280	8000.438301	10.897587	-0.049694	4.815824
242.225064	8000.471354	10.902592	-0.049669	4.815834
242.101203	8000.428784	10.907597	-0.049645	4.815822
242.160818	8000.458544	10.912602	-0.049656	4.815831
242.521592	8000.440866	10.917607	-0.049723	4.815824
242.139244	8000.432548	10.922611	-0.049652	4.815823
242.162213	8000.460650	10.927616	-0.049656	4.815831
242.355708	8000.413592	10.932621	-0.049692	4.815817
242.354543	8000.450910	10.937626	-0.049691	4.815828
242.083808	8000.432652	10.942631	-0.049641	4.815823
242.164481	8000.456349	10.947635	-0.049656	4.815830
242.384178	8000.490826	10.952640	-0.049696	4.815839
242.064529	8000.435492	10.957645	-0.049637	4.815824
242.211806	8000.457061	10.962650	-0.049664	4.815830
242.147843	8000.472021	10.967655	-0.049652	4.815835
242.041261	8000.462814	10.972659	-0.049632	4.815833
242.220771	8000.392052	10.977664	-0.049665	4.815811
242.193053	8000.440681	10.982669	-0.049660	4.815825
242.118106	8000.457598	10.987674	-0.049645	4.815831
242.312130	8000.431895	10.992679	-0.049681	4.815822
242.322614	8000.434181	10.997683	-0.049683	4.815823
242.327264	8000.426768	11.002688	-0.049684	4.815821
242.072820	8000.409840	11.007693	-0.049636	4.815817
242.134793	8000.454580	11.012698	-0.049647	4.815830
242.241543	8000.460554	11.017703	-0.049667	4.815831
242.008842	8000.443976	11.022707	-0.049624	4.815827
241.990023	8000.442589	11.027712	-0.049620	4.815827
242.117035	8000.415804	11.032717	-0.049643	4.815818
242.301194	8000.446506	11.037722	-0.049677	4.815827
242.201400	8000.421400	11.042727	-0.049659	4.815820
242.235099	8000.430464	11.047731	-0.049665	4.815822
242.339642	8000.446007	11.052736	-0.049684	4.815826
242.201968	8000.420290	11.057741	-0.049658	4.815819
242.312150	8000.456202	11.062746	-0.049679	4.815829
242.284612	8000.446136	11.067751	-0.049673	4.815827
242.231513	8000.411110	11.072755	-0.049663	4.815817
242.221062	8000.466422	11.077760	-0.049661	4.815833
242.245131	8000.404892	11.082765	-0.049665	4.815815
242.358966	8000.415249	11.087770	-0.049686	4.815817
242.285460	8000.447131	11.092775	-0.049672	4.815827
242.062800	8000.436052	11.097779	-0.049631	4.815825
242.280734	8000.472635	11.102784	-0.049671	4.815834
242.098293	8000.415245	11.107789	-0.049637	4.815818
242.077226	8000.435166	11.112794	-0.049633	4.815824
242.292191	8000.421540	11.117799	-0.049673	4.815819
242.268706	8000.465969	11.122803	-0.049668	4.815833
242.319489	8000.451829	11.127808	-0.049677	4.815828
242.156049	8000.422495	11.132813	-0.049647	4.815820
242.203755	8000.441390	11.137818	-0.049655	4.815826
242.296300	8000.471682	11.142823	-0.049672	4.815834
242.349212	8000.447971	11.147827	-0.049682	4.815827
242.395623	8000.484989	11.152832	-0.049691	4.815838
242.445014	8000.501778	11.157837	-0.049700	4.815842
242.056557	8000.404779	11.162842	-0.049627	4.815816
242.382991	8000.505012	11.167847	-0.049688	4.815843
242.163407	8000.431014	11.172851	-0.049646	4.815823
242.190605	8000.448512	11.177856	-0.049651	4.815828
242.420369	8000.443663	11.182861	-0.049694	4.815825
242.414200	8000.443546	11.187866	-0.049693	4.815825
242.080888	8000.459498	11.192871	-0.049630	4.815832
242.199677	8000.438985	11.197875	-0.049652	4.815825
242.371752	8000.471626	11.202880	-0.049684	4.815834
242.306733	8000.443879	11.207885	-0.049672	4.815826
242.358279	8000.443626	11.212890	-0.049681	4.815826
242.430304	8000.445838	11.217895	-0.049694	4.815826
242.384802	8000.425876	11.222899	-0.049686	4.815820
242.327702	8000.463359	11.227904	-0.049675	4.815832
242.230106	8000.439356	11.232909	-0.049657	4.815825
242.254969	8000.450412	11.237914	-0.049661	4.815828
242.335844	8000.453834	11.242919	-0.049676	4.815829
242.177265	8000.420309	11.247923	-0.049646	4.815820
242.360889	8000.476616	11.252928	-0.049680	4.815835
242.164586	8000.427541	11.257933	-0.049643	4.815822
242.220706	8000.445505	11.262938	-0.049654	4.815827
242.279748	8000.444305	11.267943	-0.049664	4.815826
242.256446	8000.406559	11.272947	-0.049660	4.815815
242.423468	8000.445522	11.277952	-0.049691	4.815826
242.349932	8000.411234	11.282957	-0.049677	4.815816
242.366898	8000.417894	11.287962	-0.049680	4.815818
242.363602	8000.352722	11.292967	-0.049679	4.815799
242.428547	8000.409249	11.297971	-0.049691	4.815815
242.609143	8000.432423	11.302976	-0.049724	4.815821
242.421807	8000.403770	11.307981	-0.049689	4.815814
242.299002	8000.418848	11.312986	-0.049666	4.815819
242.259144	8000.433129	11.317991	-0.049659	4.815823
242.283033	8000.407884	11.322995	-0.049663	4.815816
242.350642	8000.436705	11.328000	-0.049675	4.815824
242.392690	8000.418156	11.333005	-0.049683	4.815818
242.285749	8000.429221	11.338010	-0.049663	4.815822
242.377998	8000.431759	11.343015	-0.049680	4.815822
242.295670	8000.401598	11.348019	-0.049664	4.815814
242.538338	8000.452455	11.353024	-0.049709	4.815828
242.770825	8000.432708	11.358029	-0.049752	4.815821
242.566256	8000.417651	11.363034	-0.049714	4.815817
242.567040	8000.436857	11.368039	-0.049714	4.815823
242.545856	8000.415153	11.373043	-0.049710	4.815817
242.599431	8000.426673	11.378048	-0.049720	4.815820
242.518335	8000.404003	11.383053	-0.049704	4.815813
242.557131	8000.438764	11.388058	-0.049711	4.815823
242.590845	8000.458501	11.393063	-0.049717	4.815829
242.260489	8000.430743	11.398067	-0.049656	4.815823
242.393710	8000.463825	11.403072	-0.049680	4.815832
242.502137	8000.432472	11.408077	-0.049700	4.815822
242.490399	8000.451476	11.413082	-0.049698	4.815828
242.401231	8000.437213	11.418087	-0.049681	4.815824
242.556475	8000.413019	11.423091	-0.049710	4.815816
242.688318	8000.450348	11.428096	-0.049734	4.815826
242.509905	8000.402628	11.433101	-0.049701	4.815813
242.632826	8000.436612	11.438106	-0.049723	4.815823
242.670791	8000.461754	11.443111	-0.049730	4.815830
242.443393	8000.457001	11.448115	-0.049688	4.815829
242.563972	8000.456795	11.453120	-0.049710	4.815829
242.751210	8000.468336	11.458125	-0.049745	4.815831
242.581883	8000.436772	11.463130	-0.049713	4.815823
242.417433	8000.419160	11.468135	-0.049682	4.815818
242.359824	8000.422483	11.473139	-0.049671	4.815820
242.473423	8000.425365	11.478144	-0.049692	4.815820
242.282802	8000.399862	11.483149	-0.049656	4.815813
242.346249	8000.405137	11.488154	-0.049668	4.815815
242.448523	8000.350205	11.493159	-0.049687	4.815798
242.422029	8000.400988	11.498163	-0.049682	4.815813
242.473983	8000.433827	11.503168	-0.049691	4.815823
242.546056	8000.407224	11.508173	-0.049704	4.815814
242.423420	8000.434044	11.513178	-0.049681	4.815823
242.509786	8000.478111	11.518183	-0.049697	4.815835
242.534715	8000.417662	11.523187	-0.049702	4.815818
242.550982	8000.444589	11.528192	-0.049705	4.815825
242.383287	8000.410916	11.533197	-0.049673	4.815816
242.452950	8000.421628	11.538202	-0.049686	4.815819
242.751383	8000.453106	11.543207	-0.049741	4.815827
242.333893	8000.432481	11.548211	-0.049663	4.815823
242.571033	8000.468306	11.553216	-0.049707	4.815832
242.745996	8000.454035	11.558221	-0.049740	4.815827
242.611155	8000.434767	11.563226	-0.049714	4.815822
242.576754	8000.491827	11.568231	-0.049708	4.815839
242.412029	8000.425117	11.573235	-0.049677	4.815820
242.503709	8000.455395	11.578240	-0.049694	4.815829
242.349311	8000.455022	11.583245	-0.049665	4.815829
242.551665	8000.459336	11.588250	-0.049702	4.815830
242.640534	8000.476761	11.593255	-0.049719	4.815834
242.557428	8000.429511	11.598259	-0.049703	4.815821
242.297397	8000.466923	11.603264	-0.049654	4.815833
242.622430	8000.391037	11.608269	-0.049715	4.815809
242.602171	8000.456863	11.613274	-0.049711	4.815829
242.768104	8000.447783	11.618279	-0.049742	4.815825
242.622459	8000.439013	11.623283	-0.049714	4.815823
242.747873	8000.471969	11.628288	-0.049737	4.815833
242.440743	8000.447787	11.633293	-0.049680	4.815827
242.446568	8000.441461	11.638298	-0.049681	4.815825
242.571088	8000.490411	11.643303	-0.049704	4.815839
242.413414	8000.467573	11.648307	-0.049674	4.815833
242.208710	8000.453582	11.653312	-0.049636	4.815830
242.431981	8000.462502	11.658317	-0.049677	4.815831
242.348332	8000.435522	11.663322	-0.049662	4.815824
242.354405	8000.455880	11.668327	-0.049663	4.815830
242.501090	8000.451826	11.673331	-0.049690	4.815828
242.546263	8000.453604	11.678336	-0.049698	4.815828
242.490772	8000.413204	11.683341	-0.049687	4.815817
242.462156	8000.389246	11.688346	-0.049682	4.815810
242.765678	8000.351434	11.693351	-0.049738	4.815797
242.688108	8000.429142	11.698355	-0.049723	4.815820
242.659515	8000.443606	11.703360	-0.049718	4.815825
242.718433	8000.432799	11.708365	-0.049729	4.815821
242.489422	8000.432290	11.713370	-0.049686	4.815822
242.457240	8000.439224	11.718375	-0.049680	4.815824
242.483079	8000.425750	11.723379	-0.049684	4.815820
242.754941	8000.458934	11.728384	-0.049735	4.815829
242.831958	8000.434545	11.733389	-0.049749	4.815821
242.594976	8000.443512	11.738394	-0.049705	4.815825
242.808112	8000.473615	11.743399	-0.049744	4.815833
242.892437	8000.434402	11.748403	-0.049760	4.815821
242.585622	8000.462521	11.753408	-0.049702	4.815831
242.570553	8000.415301	11.758413	-0.049699	4.815817
242.546095	8000.415957	11.763418	-0.049694	4.815817
242.444622	8000.451657	11.768423	-0.049675	4.815828
242.435840	8000.426951	11.773427	-0.049674	4.815821
242.771338	8000.460095	11.778432	-0.049736	4.815829
242.765015	8000.488792	11.783437	-0.049734	4.815838
242.447990	8000.439903	11.788442	-0.049675	4.815825
242.560392	8000.470515	11.793447	-0.049696	4.815833
242.806857	8000.424312	11.798451	-0.049742	4.815818
242.579021	8000.357652	11.803456	-0.049699	4.815800
242.578006	8000.426990	11.808461	-0.049699	4.815820
242.534382	8000.416664	11.813466	-0.049690	4.815818
242.526305	8000.422920	11.818471	-0.049689	4.815819
242.434782	8000.407552	11.823475	-0.049671	4.815815
242.659116	8000.464517	11.828480	-0.049713	4.815831
242.545008	8000.464793	11.833485	-0.049691	4.815832
242.316760	8000.448288	11.838490	-0.049649	4.815828
242.560172	8000.451129	11.843495	-0.049694	4.815828
242.591996	8000.427079	11.848499	-0.049700	4.815820
242.602641	8000.443242	11.853504	-0.049701	4.815825
242.531751	8000.438880	11.858509	-0.049688	4.815824
242.571763	8000.440575	11.863514	-0.049695	4.815824
242.733280	8000.458105	11.868519	-0.049725	4.815829
242.591096	8000.440853	11.873523	-0.049698	4.815824
242.673383	8000.467777	11.878528	-0.049714	4.815832
242.805103	8000.473087	11.883533	-0.049738	4.815833
242.416714	8000.453998	11.888538	-0.049665	4.815829
242.510310	8000.498180	11.893543	-0.049683	4.815842
242.590029	8000.465297	11.898547	-0.049697	4.815832
242.521380	8000.389465	11.903552	-0.049684	4.815810
242.654746	8000.455634	11.908557	-0.049709	4.815828
242.526429	8000.429000	11.913562	-0.049685	4.815821
242.874711	8000.469821	11.918567	-0.049750	4.815832
242.709519	8000.446861	11.923571	-0.049719	4.815826
242.878513	8000.491193	11.928576	-0.049750	4.815838
242.753953	8000.491301	11.933581	-0.049726	4.815838
242.508584	8000.441434	11.938586	-0.049681	4.815825
242.709212	8000.437182	11.943591	-0.049718	4.815823
242.804058	8000.423754	11.948595	-0.049735	4.815818
242.828584	8000.463621	11.953600	-0.049740	4.815830
242.693968	8000.432616	11.958605	-0.049714	4.815822
242.702016	8000.442334	11.963610	-0.049716	4.815824
242.779191	8000.470243	11.968615	-0.049730	4.815832
242.715587	8000.449990	11.973619	-0.049718	4.815827
242.578283	8000.453094	11.978624	-0.049692	4.815828
242.678840	8000.372520	11.983629	-0.049710	4.815804
242.791470	8000.435153	11.988634	-0.049731	4.815822
242.847851	8000.445651	11.993639	-0.049742	4.815825
242.588774	8000.405168	11.998643	-0.049693	4.815814
242.748981	8000.445089	12.003648	-0.049723	4.815825
242.817072	8000.418422	12.008653	-0.049735	4.815817
242.765661	8000.432517	12.013658	-0.049725	4.815821
242.704490	8000.480607	12.018663	-0.049714	4.815836
242.652895	8000.434933	12.023667	-0.049704	4.815823
242.968633	8000.447480	12.028672	-0.049763	4.815825
242.813901	8000.467379	12.033677	-0.049734	4.815831
242.686366	8000.434354	12.038682	-0.049710	4.815822
242.816888	8000.452451	12.043687	-0.049734	4.815827
242.827484	8000.422722	12.048691	-0.049736	4.815818
242.845656	8000.481697	12.053696	-0.049739	4.815835
242.738416	8000.473547	12.058701	-0.049719	4.815833
242.755532	8000.444989	12.063706	-0.049722	4.815825
242.823395	8000.468480	12.068711	-0.049734	4.815832
242.712909	8000.429326	12.073715	-0.049713	4.815821
242.569917	8000.373640	12.078720	-0.049686	4.815805
242.794307	8000.414596	12.083725	-0.049728	4.815816
242.562852	8000.431123	12.088730	-0.049685	4.815822
242.765162	8000.478127	12.093735	-0.049722	4.815835
242.582564	8000.458088	12.098739	-0.049688	4.815830
242.545947	8000.452144	12.103744	-0.049681	4.815828
242.820503	8000.441614	12.108749	-0.049732	4.815824
242.775405	8000.418457	12.113754	-0.049723	4.815817
242.778910	8000.453716	12.118759	-0.049724	4.815828
242.651446	8000.437769	12.123763	-0.049700	4.815823
242.777653	8000.446191	12.128768	-0.049723	4.815825
242.875549	8000.444551	12.133773	-0.049741	4.815824
242.581547	8000.434455	12.138778	-0.049686	4.815823
242.485115	8000.444623	12.143783	-0.049668	4.815826
242.508102	8000.407623	12.148787	-0.049672	4.815815
242.765096	8000.452306	12.153792	-0.049720	4.815827
242.573030	8000.427846	12.158797	-0.049684	4.815821
242.716213	8000.421600	12.163802	-0.049710	4.815818
242.757475	8000.462805	12.168807	-0.049718	4.815830
242.625123	8000.436106	12.173811	-0.049693	4.815823
242.654959	8000.470722	12.178816	-0.049698	4.815833
242.835513	8000.363690	12.183821	-0.049732	4.815801
242.866780	8000.423944	12.188826	-0.049737	4.815818
242.768996	8000.445829	12.193831	-0.049719	4.815825
242.777483	8000.487572	12.198835	-0.049720	4.815838
242.808060	8000.490183	12.203840	-0.049726	4.815838
242.919058	8000.495158	12.208845	-0.049746	4.815839
242.610555	8000.451743	12.213850	-0.049689	4.815828
242.899923	8000.385954	12.218855	-0.049742	4.815807
242.616015	8000.441124	12.223859	-0.049689	4.815825
242.635960	8000.442496	12.228864	-0.049693	4.815825
242.995473	8000.478162	12.233869	-0.049760	4.815834
242.824540	8000.418822	12.238874	-0.049728	4.815817
242.569404	8000.457380	12.243879	-0.049680	4.815830
242.450551	8000.428764	12.248883	-0.049657	4.815822
242.910158	8000.437228	12.253888	-0.049743	4.815822
242.868993	8000.428009	12.258893	-0.049735	4.815820
242.642318	8000.426470	12.263898	-0.049693	4.815820
243.000962	8000.470660	12.268903	-0.049759	4.815832
242.969434	8000.462663	12.273907	-0.049753	4.815829
242.837446	8000.496803	12.278912	-0.049728	4.815840
242.905039	8000.425303	12.283917	-0.049741	4.815819
242.794808	8000.425642	12.288922	-0.049720	4.815819
242.720715	8000.483129	12.293927	-0.049706	4.815837
242.773305	8000.424194	12.298931	-0.049716	4.815819
242.895942	8000.457106	12.303936	-0.049738	4.815828
242.840272	8000.490343	12.308941	-0.049728	4.815838
242.690664	8000.461231	12.313946	-0.049700	4.815830
242.938177	8000.504695	12.318951	-0.049746	4.815842
242.731512	8000.452250	12.323955	-0.049707	4.815828
242.794682	8000.431907	12.328960	-0.049718	4.815821
242.846397	8000.435926	12.333965	-0.049728	4.815822
242.908721	8000.432645	12.338970	-0.049739	4.815821
243.027237	8000.370504	12.343975	-0.049761	4.815802
243.005781	8000.449118	12.348979	-0.049757	4.815825
243.166553	8000.462367	12.353984	-0.049787	4.815828
243.144415	8000.443850	12.358989	-0.049782	4.815823
243.051148	8000.432722	12.363994	-0.049765	4.815820
243.134142	8000.474600	12.368999	-0.049780	4.815832
242.970380	8000.432452	12.374003	-0.049749	4.815821
242.847968	8000.440066	12.379008	-0.049726	4.815823
243.049521	8000.456107	12.384013	-0.049764	4.815827
243.034138	8000.416353	12.389018	-0.049761	4.815816
242.935352	8000.462769	12.394023	-0.049742	4.815830
242.646608	8000.417539	12.399027	-0.049688	4.815818
242.786337	8000.447524	12.404032	-0.049714	4.815826
242.962019	8000.452476	12.409037	-0.049746	4.815827
242.635469	8000.400232	12.414042	-0.049685	4.815813
242.893162	8000.447062	12.419047	-0.049733	4.815825
242.957777	8000.418204	12.424051	-0.049745	4.815817
242.710140	8000.432335	12.429056	-0.049699	4.815822
242.765563	8000.439616	12.434061	-0.049709	4.815824
242.716817	8000.426005	12.439066	-0.049700	4.815820
242.925488	8000.444296	12.444071	-0.049738	4.815824
242.692850	8000.409576	12.449075	-0.049695	4.815815
242.958971	8000.436264	12.454080	-0.049744	4.815822
242.949258	8000.430753	12.459085	-0.049742	4.815820
242.847904	8000.402420	12.464090	-0.049723	4.815813
242.979616	8000.357568	12.469095	-0.049747	4.815799
243.096524	8000.418136	12.474099	-0.049769	4.815816
243.033343	8000.441647	12.479104	-0.049757	4.815823
242.826944	8000.432964	12.484109	-0.049718	4.815822
242.799480	8000.409024	12.489114	-0.049713	4.815815
242.904303	8000.441648	12.494119	-0.049732	4.815824
243.079877	8000.425253	12.499123	-0.049765	4.815818
242.828662	8000.443596	12.504128	-0.049718	4.815825
242.991844	8000.449413	12.509133	-0.049748	4.815826
242.776931	8000.425651	12.514138	-0.049708	4.815820
242.964184	8000.447865	12.519143	-0.049742	4.815825
243.054071	8000.429020	12.524147	-0.049759	4.815819
242.964121	8000.428619	12.529152	-0.049742	4.815820
242.999197	8000.440908	12.534157	-0.049748	4.815823
242.843773	8000.419173	12.539162	-0.049719	4.815818
242.777190	8000.441561	12.544167	-0.049707	4.815824
242.675664	8000.424965	12.549171	-0.049688	4.815820
242.821448	8000.424097	12.554176	-0.049714	4.815819
243.127403	8000.462101	12.559181	-0.049771	4.815829
242.684974	8000.418660	12.564186	-0.049689	4.815818
243.011957	8000.429254	12.569191	-0.049749	4.815820
242.965827	8000.386869	12.574195	-0.049741	4.815808
242.985839	8000.436269	12.579200	-0.049744	4.815822
242.896637	8000.439082	12.584205	-0.049727	4.815823
242.690564	8000.419732	12.589210	-0.049689	4.815818
242.745445	8000.447281	12.594215	-0.049699	4.815826
242.745914	8000.421658	12.599219	-0.049699	4.815819
242.725625	8000.413843	12.604224	-0.049695	4.815817
242.964531	8000.424083	12.609229	-0.049739	4.815818
242.907383	8000.423144	12.614234	-0.049728	4.815818
242.727891	8000.451182	12.619239	-0.049695	4.815828
242.768030	8000.349356	12.624243	-0.049702	4.815798
242.808949	8000.451388	12.629248	-0.049709	4.815827
242.906294	8000.449739	12.634253	-0.049727	4.815826
242.905072	8000.413416	12.639258	-0.049727	4.815816
243.016085	8000.436534	12.644263	-0.049747	4.815822
242.944892	8000.428965	12.649267	-0.049734	4.815820
242.878204	8000.458823	12.654272	-0.049721	4.815829
242.844779	8000.431585	12.659277	-0.049715	4.815821
243.045550	8000.401722	12.664282	-0.049752	4.815812
242.988469	8000.426398	12.669287	-0.049741	4.815819
243.028874	8000.398217	12.674291	-0.049748	4.815811
243.054826	8000.412493	12.679296	-0.049753	4.815815
242.868164	8000.430810	12.684301	-0.049718	4.815821
242.819885	8000.395861	12.689306	-0.049709	4.815811
243.065243	8000.433954	12.694311	-0.049754	4.815821
243.193744	8000.415732	12.699315	-0.049778	4.815815
243.017019	8000.402192	12.704320	-0.049745	4.815812
243.088733	8000.425744	12.709325	-0.049758	4.815818
242.832451	8000.409853	12.714330	-0.049710	4.815815
242.906658	8000.447320	12.719335	-0.049724	4.815826
242.943735	8000.426555	12.724339	-0.049731	4.815819
243.030906	8000.420474	12.729344	-0.049747	4.815817
242.816834	8000.410600	12.734349	-0.049706	4.815815
242.748818	8000.400948	12.739354	-0.049694	4.815813
242.830738	8000.435337	12.744359	-0.049709	4.815823
242.738459	8000.389006	12.749363	-0.049691	4.815809
242.709697	8000.414140	12.754368	-0.049686	4.815817
243.002206	8000.439119	12.759373	-0.049740	4.815823
242.833814	8000.417175	12.764378	-0.049708	4.815817
242.814988	8000.402979	12.769383	-0.049705	4.815813
242.971427	8000.396948	12.774387	-0.049734	4.815811
242.915543	8000.416307	12.779392	-0.049723	4.815817
242.838160	8000.418243	12.784397	-0.049708	4.815818
242.794814	8000.403653	12.789402	-0.049700	4.815813
243.214953	8000.438162	12.794407	-0.049778	4.815822
242.933732	8000.414397	12.799411	-0.049726	4.815816
242.822132	8000.416849	12.804416	-0.049705	4.815817
243.009662	8000.434799	12.809421	-0.049739	4.815822
243.002696	8000.415458	12.814426	-0.049738	4.815816
242.957785	8000.421120	12.819431	-0.049729	4.815818
242.916665	8000.399095	12.824435	-0.049722	4.815812
242.986213	8000.413007	12.829440	-0.049734	4.815815
243.090317	8000.471234	12.834445	-0.049754	4.815832
242.841516	8000.413840	12.839450	-0.049707	4.815816
242.969198	8000.450035	12.844455	-0.049731	4.815826
242.945567	8000.438964	12.849459	-0.049726	4.815823
242.867267	8000.448356	12.854464	-0.049711	4.815826
243.125360	8000.433292	12.859469	-0.049759	4.815821
243.079708	8000.403722	12.864474	-0.049750	4.815812
243.124338	8000.410829	12.869479	-0.049758	4.815814
242.904399	8000.393390	12.874483	-0.049717	4.815810
243.154241	8000.423017	12.879488	-0.049764	4.815818
243.170376	8000.449942	12.884493	-0.049766	4.815825
242.867726	8000.403419	12.889498	-0.049710	4.815813
243.029695	8000.344114	12.894503	-0.049740	4.815795
243.112360	8000.450022	12.899507	-0.049755	4.815826
243.221824	8000.436829	12.904512	-0.049775	4.815821
242.986338	8000.429811	12.909517	-0.049731	4.815820
243.132373	8000.409737	12.914522	-0.049758	4.815814
243.177243	8000.445664	12.919527	-0.049766	4.815824
242.941933	8000.395958	12.924531	-0.049722	4.815811
242.931045	8000.411774	12.929536	-0.049720	4.815815
242.949515	8000.422728	12.934541	-0.049723	4.815818
242.865523	8000.411751	12.939546	-0.049707	4.815816
243.016127	8000.425903	12.944551	-0.049735	4.815819
243.085199	8000.440874	12.949555	-0.049748	4.815823
243.174764	8000.439100	12.954560	-0.049764	4.815822
243.260284	8000.440463	12.959565	-0.049780	4.815822
243.376850	8000.426317	12.964570	-0.049802	4.815818
243.309078	8000.451888	12.969575	-0.049789	4.815825
243.104587	8000.414420	12.974579	-0.049751	4.815815
243.325125	8000.410490	12.979584	-0.049791	4.815813
243.246806	8000.447631	12.984589	-0.049777	4.815824
242.960102	8000.403500	12.989594	-0.049723	4.815813
242.946010	8000.436340	12.994599	-0.049720	4.815823
243.048992	8000.418774	12.999603	-0.049739	4.815817
242.925491	8000.423168	13.004608	-0.049716	4.815819
242.955283	8000.440708	13.009613	-0.049721	4.815824
242.950049	8000.397916	13.014618	-0.049720	4.815811
243.003354	8000.433978	13.019623	-0.049730	4.815822
242.906551	8000.430265	13.024627	-0.049712	4.815821
242.974036	8000.434538	13.029632	-0.049724	4.815822
243.165754	8000.438681	13.034637	-0.049760	4.815822
242.975975	8000.427064	13.039642	-0.049724	4.815820
243.131055	8000.479710	13.044647	-0.049753	4.815834
243.252887	8000.390941	13.049651	-0.049775	4.815808
242.933902	8000.445545	13.054656	-0.049716	4.815825
242.976421	8000.456886	13.059661	-0.049723	4.815828
242.898207	8000.434262	13.064666	-0.049709	4.815822
243.050862	8000.476196	13.069671	-0.049737	4.815834
243.036433	8000.440727	13.074675	-0.049734	4.815823
242.961706	8000.446975	13.079680	-0.049720	4.815826
242.945859	8000.449904	13.084685	-0.049717	4.815827
242.825116	8000.399913	13.089690	-0.049694	4.815813
242.831065	8000.425606	13.094695	-0.049695	4.815820
243.045099	8000.423705	13.099699	-0.049735	4.815818
242.990664	8000.440953	13.104704	-0.049724	4.815824
243.011646	8000.438073	13.109709	-0.049728	4.815823
243.000540	8000.441078	13.114714	-0.049726	4.815824
243.102456	8000.458714	13.119719	-0.049745	4.815828
243.060168	8000.418526	13.124723	-0.049736	4.815817
243.048831	8000.405519	13.129728	-0.049734	4.815813
243.167707	8000.442639	13.134733	-0.049756	4.815823
243.000198	8000.407902	13.139738	-0.049725	4.815814
243.194596	8000.424895	13.144743	-0.049761	4.815818
243.183502	8000.424699	13.149747	-0.049758	4.815818
242.966729	8000.423320	13.154752	-0.049718	4.815819
243.041077	8000.435174	13.159757	-0.049731	4.815822
243.231089	8000.373120	13.164762	-0.049767	4.815803
243.137875	8000.451643	13.169767	-0.049749	4.815826
243.039205	8000.427622	13.174771	-0.049731	4.815820
242.905457	8000.425448	13.179776	-0.049705	4.815820
243.107605	8000.443633	13.184781	-0.049743	4.815824
243.107697	8000.428676	13.189786	-0.049743	4.815820
243.078489	8000.453802	13.194791	-0.049737	4.815827
243.291262	8000.378240	13.199795	-0.049776	4.815804
243.099275	8000.450901	13.204800	-0.049741	4.815826
243.177314	8000.456412	13.209805	-0.049755	4.815828
243.214556	8000.426045	13.214810	-0.049762	4.815818
243.247271	8000.469246	13.219815	-0.049768	4.815831
243.103070	8000.474373	13.224819	-0.049740	4.815833
243.083694	8000.437757	13.229824	-0.049737	4.815823
243.200325	8000.465236	13.234829	-0.049758	4.815830
243.092077	8000.422916	13.239834	-0.049738	4.815818
243.164281	8000.426198	13.244839	-0.049751	4.815819
243.236381	8000.422008	13.249843	-0.049764	4.815817
243.167785	8000.428355	13.254848	-0.049751	4.815819
242.942939	8000.457796	13.259853	-0.049709	4.815829
243.169476	8000.409138	13.264858	-0.049751	4.815814
243.406017	8000.428945	13.269863	-0.049795	4.815818
243.152546	8000.440848	13.274867	-0.049748	4.815823
243.040362	8000.415541	13.279872	-0.049727	4.815816
243.290147	8000.371527	13.284877	-0.049773	4.815802
243.199235	8000.413801	13.289882	-0.049756	4.815815
243.349502	8000.434352	13.294887	-0.049784	4.815820
243.402781	8000.455472	13.299891	-0.049793	4.815826
243.245396	8000.425167	13.304896	-0.049764	4.815818
243.117022	8000.436953	13.309901	-0.049740	4.815822
243.149692	8000.410782	13.314906	-0.049746	4.815814
243.290461	8000.450390	13.319911	-0.049772	4.815825
243.202385	8000.430808	13.324915	-0.049755	4.815820
242.969430	8000.419562	13.329920	-0.049711	4.815818
243.098073	8000.442966	13.334925	-0.049735	4.815824
243.090695	8000.414013	13.339930	-0.049734	4.815816
243.355476	8000.456689	13.344935	-0.049783	4.815827
243.300660	8000.470730	13.349939	-0.049772	4.815831
243.176915	8000.417487	13.354944	-0.049749	4.815816
243.184570	8000.457083	13.359949	-0.049750	4.815828
243.076611	8000.414768	13.364954	-0.049730	4.815816
243.096557	8000.438552	13.369959	-0.049734	4.815823
242.997980	8000.410264	13.374963	-0.049715	4.815815
243.024818	8000.410679	13.379968	-0.049720	4.815815
243.168989	8000.451409	13.384973	-0.049746	4.815826
243.171428	8000.432221	13.389978	-0.049747	4.815821
243.003485	8000.439100	13.394983	-0.049715	4.815823
243.161511	8000.451237	13.399987	-0.049744	4.815826
243.039903	8000.431115	13.404992	-0.049722	4.815821
243.054070	8000.444134	13.409997	-0.049724	4.815825
242.941448	8000.446569	13.415002	-0.049703	4.815826
242.910489	8000.463128	13.420007	-0.049697	4.815831
242.986948	8000.433394	13.425011	-0.049711	4.815822
242.841341	8000.413952	13.430016	-0.049684	4.815817
243.050443	8000.458931	13.435021	-0.049722	4.815829
242.955694	8000.414695	13.440026	-0.049704	4.815817
242.960307	8000.425425	13.445031	-0.049705	4.815820
243.153552	8000.464812	13.450035	-0.049741	4.815830
242.935124	8000.442061	13.455040	-0.049700	4.815825
242.890816	8000.365554	13.460045	-0.049692	4.815803
242.915222	8000.394746	13.465050	-0.049696	4.815811
243.112173	8000.438462	13.470055	-0.049732	4.815823
243.164302	8000.421142	13.475059	-0.049742	4.815818
243.073697	8000.413260	13.480064	-0.049725	4.815816
243.059624	8000.463177	13.485069	-0.049722	4.815830
243.038298	8000.422260	13.490074	-0.049718	4.815818
242.888177	8000.442234	13.495079	-0.049690	4.815825
242.853214	8000.427779	13.500083	-0.049683	4.815821
243.041522	8000.417992	13.505088	-0.049718	4.815817
243.055502	8000.424604	13.510093	-0.049720	4.815819
243.113751	8000.410585	13.515098	-0.049731	4.815815
243.147143	8000.410039	13.520103	-0.049737	4.815814
243.207648	8000.417401	13.525107	-0.049748	4.815816
243.104641	8000.442404	13.530112	-0.049729	4.815824
243.167579	8000.488227	13.535117	-0.049740	4.815837
243.178501	8000.447830	13.540122	-0.049742	4.815825
243.285383	8000.468748	13.545127	-0.049762	4.815831
243.026994	8000.441083	13.550131	-0.049713	4.815824
243.186737	8000.441508	13.555136	-0.049743	4.815823
243.258013	8000.455448	13.560141	-0.049756	4.815827
243.240343	8000.402850	13.565146	-0.049753	4.815812
243.213523	8000.434418	13.570151	-0.049747	4.815821
243.345434	8000.445067	13.575155	-0.049772	4.815824
243.049468	8000.449881	13.580160	-0.049716	4.815827
243.090385	8000.462264	13.585165	-0.049724	4.815830
243.177668	8000.439108	13.590170	-0.049740	4.815823
243.167715	8000.389836	13.595175	-0.049738	4.815808
243.058981	8000.426486	13.600179	-0.049717	4.815820
243.084828	8000.418348	13.605184	-0.049722	4.815817
243.406730	8000.451273	13.610189	-0.049782	4.815825
243.181035	8000.431606	13.615194	-0.049740	4.815821
243.271996	8000.450132	13.620199	-0.049756	4.815826
243.332973	8000.427619	13.625203	-0.049767	4.815819
243.218528	8000.434294	13.630208	-0.049746	4.815821
243.194411	8000.472309	13.635213	-0.049741	4.815833
243.166243	8000.424878	13.640218	-0.049736	4.815819
243.415621	8000.482247	13.645223	-0.049782	4.815834
243.320801	8000.405992	13.650227	-0.049764	4.815813
243.281744	8000.453371	13.655232	-0.049757	4.815827
243.089824	8000.439585	13.660237	-0.049721	4.815823
243.037642	8000.426987	13.665242	-0.049711	4.815820
243.161638	8000.468458	13.670247	-0.049734	4.815832
243.355893	8000.473710	13.675251	-0.049770	4.815832
243.158142	8000.441686	13.680256	-0.049733	4.815824
243.287171	8000.452289	13.685261	-0.049757	4.815826
243.279591	8000.428670	13.690266	-0.049755	4.815819
243.124624	8000.441094	13.695271	-0.049726	4.815824
243.125314	8000.434685	13.700275	-0.049726	4.815822
243.161636	8000.405370	13.705280	-0.049732	4.815813
243.196835	8000.367500	13.710285	-0.049739	4.815802
243.169705	8000.435349	13.715290	-0.049733	4.815822
243.217580	8000.451046	13.720295	-0.049742	4.815826
243.218009	8000.467045	13.725299	-0.049742	4.815831
243.099159	8000.429891	13.730304	-0.049720	4.815821
243.227702	8000.459696	13.735309	-0.049744	4.815829
243.176695	8000.440713	13.740314	-0.049734	4.815823
243.232242	8000.450130	13.745319	-0.049744	4.815826
243.196163	8000.454867	13.750323	-0.049737	4.815828
243.097792	8000.420178	13.755328	-0.049719	4.815818
243.196145	8000.445227	13.760333	-0.049737	4.815825
242.976175	8000.413913	13.765338	-0.049695	4.815817
243.185760	8000.433286	13.770343	-0.049734	4.815821
243.532406	8000.477283	13.775347	-0.049799	4.815833
243.140896	8000.436797	13.780352	-0.049726	4.815823
243.241468	8000.486429	13.785357	-0.049744	4.815837
243.338207	8000.418600	13.790362	-0.049762	4.815816
243.431081	8000.437158	13.795367	-0.049779	4.815821
243.361130	8000.463761	13.800371	-0.049766	4.815829
243.253750	8000.375563	13.805376	-0.049746	4.815804
243.439432	8000.457519	13.810381	-0.049780	4.815827
243.092289	8000.443364	13.815386	-0.049715	4.815825
243.164062	8000.427428	13.820391	-0.049728	4.815820
243.268085	8000.419484	13.825395	-0.049747	4.815817
243.109746	8000.437190	13.830400	-0.049718	4.815823
243.073828	8000.463275	13.835405	-0.049711	4.815831
243.096123	8000.429466	13.840410	-0.049715	4.815821
243.209097	8000.431271	13.845415	-0.049736	4.815821
243.254117	8000.454392	13.850419	-0.049744	4.815827
243.288033	8000.453855	13.855424	-0.049750	4.815827
243.540479	8000.472853	13.860429	-0.049797	4.815831
243.361639	8000.464614	13.865434	-0.049763	4.815830
243.165194	8000.448620	13.870439	-0.049727	4.815826
243.213204	8000.470723	13.875443	-0.049735	4.815832
243.317039	8000.456372	13.880448	-0.049754	4.815828
243.335868	8000.357403	13.885453	-0.049758	4.815798
243.407246	8000.417237	13.890458	-0.049771	4.815816
243.481123	8000.458968	13.895463	-0.049784	4.815828
243.322552	8000.468132	13.900467	-0.049755	4.815831
243.129382	8000.422309	13.905472	-0.049718	4.815818
243.381151	8000.470111	13.910477	-0.049765	4.815831
243.270778	8000.443766	13.915482	-0.049744	4.815824
243.040921	8000.445377	13.920487	-0.049701	4.815826
243.268810	8000.519476	13.925491	-0.049744	4.815846
243.384583	8000.447685	13.930496	-0.049765	4.815825
243.391071	8000.446705	13.935501	-0.049766	4.815824
243.395478	8000.456365	13.940506	-0.049767	4.815827
243.393313	8000.449909	13.945511	-0.049766	4.815825
243.489741	8000.425833	13.950515	-0.049784	4.815818
243.201406	8000.421165	13.955520	-0.049730	4.815818
243.411933	8000.440553	13.960525	-0.049769	4.815823
243.427017	8000.446115	13.965530	-0.049772	4.815824
243.322397	8000.452949	13.970535	-0.049752	4.815827
243.296235	8000.431164	13.975539	-0.049747	4.815820
243.239734	8000.447312	13.980544	-0.049736	4.815825
243.172987	8000.471832	13.985549	-0.049723	4.815833
243.271519	8000.468068	13.990554	-0.049742	4.815831
243.275626	8000.443570	13.995559	-0.049742	4.815824
243.495824	8000.484460	14.000563	-0.049783	4.815835
243.114523	8000.431332	14.005568	-0.049712	4.815821
243.259263	8000.444322	14.010573	-0.049739	4.815824
243.297786	8000.429985	14.015578	-0.049745	4.815820
243.257781	8000.441062	14.020583	-0.049738	4.815823
243.472515	8000.426366	14.025587	-0.049778	4.815818
243.223722	8000.411663	14.030592	-0.049731	4.815815
243.596599	8000.446477	14.035597	-0.049800	4.815823
243.393496	8000.371677	14.040602	-0.049762	4.815803
243.405729	8000.480718	14.045607	-0.049764	4.815834
243.436531	8000.516418	14.050611	-0.049770	4.815845
243.338197	8000.441173	14.055616	-0.049751	4.815823
243.344562	8000.467940	14.060621	-0.049752	4.815831
243.406399	8000.424095	14.065626	-0.049764	4.815818
243.160652	8000.429719	14.070631	-0.049718	4.815821
243.266845	8000.452760	14.075635	-0.049737	4.815827
243.247701	8000.402273	14.080640	-0.049734	4.815812
243.281205	8000.392124	14.085645	-0.049740	4.815809
243.262903	8000.437704	14.090650	-0.049736	4.815823
243.223946	8000.456269	14.095655	-0.049729	4.815828
243.517181	8000.468453	14.100659	-0.049783	4.815830
243.117060	8000.433165	14.105664	-0.049708	4.815822
243.295294	8000.472310	14.110669	-0.049741	4.815833
243.383351	8000.467310	14.115674	-0.049757	4.815831
243.209062	8000.446338	14.120679	-0.049725	4.815825
243.266274	8000.451513	14.125683	-0.049735	4.815827
243.259348	8000.405492	14.130688	-0.049734	4.815813
243.406191	8000.446265	14.135693	-0.049761	4.815824
243.204810	8000.410981	14.140698	-0.049723	4.815815
243.127606	8000.339280	14.145703	-0.049709	4.815794
243.166504	8000.442347	14.150707	-0.049716	4.815824
243.056797	8000.442694	14.155712	-0.049695	4.815825
243.315568	8000.451121	14.160717	-0.049743	4.815826
243.445431	8000.432921	14.165722	-0.049767	4.815820
243.338666	8000.423710	14.170727	-0.049747	4.815818
243.415275	8000.478292	14.175731	-0.049761	4.815834
243.379062	8000.454211	14.180736	-0.049754	4.815827
243.480596	8000.468639	14.185741	-0.049773	4.815831
243.408171	8000.446108	14.190746	-0.049759	4.815824
243.442109	8000.439168	14.195751	-0.049765	4.815822
243.331680	8000.421360	14.200755	-0.049744	4.815818
243.261721	8000.412744	14.205760	-0.049731	4.815815
243.553684	8000.459060	14.210765	-0.049785	4.815828
243.642523	8000.470082	14.215770	-0.049802	4.815830
243.522532	8000.399824	14.220775	-0.049779	4.815810
243.311815	8000.539421	14.225779	-0.049740	4.815852
243.196501	8000.464969	14.230784	-0.049718	4.815831
243.360825	8000.406769	14.235789	-0.049749	4.815813
243.177744	8000.442220	14.240794	-0.049714	4.815824
243.278574	8000.433157	14.245799	-0.049733	4.815821
243.316473	7999.496722	14.250803	-0.049739	4.815547

243.241936	7996.170451	14.255808	-0.049723	4.814574
243.269990	7990.651242	14.260813	-0.049724	4.812959
243.306039	7983.955829	14.265818	-0.049726	4.810999
243.069540	7976.610933	14.270823	-0.049677	4.808849
243.180592	7969.040409	14.275827	-0.049693	4.806630
243.268395	7961.203622	14.280832	-0.049704	4.804332
243.185137	7953.377574	14.285837	-0.049683	4.802037
243.070057	7945.384647	14.290842	-0.049656	4.799692
243.106276	7937.412773	14.295847	-0.049658	4.797352
243.066886	7929.463886	14.300851	-0.049645	4.795017
243.056471	7921.395039	14.305856	-0.049638	4.792646
242.996678	7913.414432	14.310861	-0.049621	4.790300
243.078406	7905.412137	14.315866	-0.049631	4.787945
243.000766	7897.373403	14.320871	-0.049611	4.785580
243.108466	7889.435516	14.325875	-0.049626	4.783242
243.194736	7881.385709	14.330880	-0.049636	4.780870
243.133650	7873.415253	14.335885	-0.049620	4.778521
242.862522	7865.417468	14.340890	-0.049564	4.776164
242.765629	7857.415372	14.345895	-0.049540	4.773803
242.874443	7849.376495	14.350899	-0.049555	4.771430
242.739345	7841.376636	14.355904	-0.049524	4.769068
242.753920	7833.383667	14.360909	-0.049522	4.766706
242.914660	7825.359448	14.365914	-0.049546	4.764333
242.764497	7817.427346	14.370919	-0.049513	4.761988
242.793182	7809.400020	14.375923	-0.049513	4.759612
242.599316	7801.401590	14.380928	-0.049471	4.757245
242.695092	7793.337742	14.385933	-0.049484	4.754856
242.824110	7785.372015	14.390938	-0.049502	4.752495
242.630008	7777.261472	14.395943	-0.049461	4.750090
242.491745	7769.312472	14.400947	-0.049430	4.747733
242.283132	7761.298402	14.405952	-0.049385	4.745355
242.356758	7753.395357	14.410957	-0.049394	4.743007
242.247190	7745.376721	14.415962	-0.049368	4.740625
242.365928	7737.339196	14.420967	-0.049385	4.738236
242.330966	7729.345148	14.425971	-0.049373	4.735858
242.155215	7721.343326	14.430976	-0.049334	4.733478
242.224405	7713.315355	14.435981	-0.049342	4.731088
242.370255	7705.316214	14.440986	-0.049364	4.728705
242.188148	7697.281517	14.445991	-0.049324	4.726311
242.329835	7689.289346	14.450995	-0.049345	4.723927
242.153138	7681.318366	14.456000	-0.049307	4.721550
242.129909	7673.287901	14.461005	-0.049297	4.719153
242.261743	7665.393430	14.466010	-0.049316	4.716795
242.093404	7657.287397	14.471015	-0.049280	4.714374
242.102861	7649.312259	14.476019	-0.049276	4.711990
241.967389	7641.254506	14.481024	-0.049245	4.709580
242.048319	7633.307859	14.486029	-0.049255	4.707202
242.015365	7625.271614	14.491034	-0.049243	4.704797
241.870043	7617.296041	14.496039	-0.049211	4.702408
242.022917	7609.348446	14.501043	-0.049234	4.700026
242.001357	7601.327710	14.506048	-0.049225	4.697621
241.700274	7593.303100	14.511053	-0.049163	4.695214
241.905531	7585.322208	14.516058	-0.049196	4.692818
241.713758	7577.242165	14.521063	-0.049155	4.690392
241.823637	7569.340548	14.526067	-0.049170	4.688018
241.591771	7561.263471	14.531072	-0.049121	4.685590
241.668323	7553.317885	14.536077	-0.049130	4.683200
241.746906	7545.300627	14.541082	-0.049139	4.680788
241.440631	7537.300100	14.546087	-0.049077	4.678379
241.499867	7529.324199	14.551091	-0.049083	4.675977
241.344219	7521.207461	14.556096	-0.049048	4.673531
241.257287	7513.151232	14.561101	-0.049026	4.671101
241.429179	7505.219281	14.566106	-0.049053	4.668708
241.406055	7497.203713	14.571111	-0.049043	4.666289
241.418855	7489.238960	14.576115	-0.049040	4.663883
241.188476	7481.268157	14.581120	-0.048992	4.661475
241.338569	7473.247107	14.586125	-0.049015	4.659050
241.409593	7465.263983	14.591130	-0.049022	4.656635
241.202995	7457.242900	14.596135	-0.048979	4.654207
241.275370	7449.255731	14.601139	-0.048987	4.651789
241.303928	7441.197377	14.606144	-0.048986	4.649347
241.373377	7433.222637	14.611149	-0.048994	4.646930
241.214184	7425.198008	14.616154	-0.048959	4.644496
241.182238	7417.240657	14.621159	-0.048948	4.642082
241.212969	7409.212533	14.626163	-0.048948	4.639644
241.082935	7401.247958	14.631168	-0.048918	4.637225
241.253308	7393.211008	14.636173	-0.048945	4.634783
241.148898	7385.215873	14.641178	-0.048920	4.632351
241.084134	7377.180913	14.646183	-0.048902	4.629907
240.932306	7369.222955	14.651187	-0.048869	4.627485
241.028138	7361.180239	14.656192	-0.048881	4.625035
241.053049	7353.190886	14.661197	-0.048880	4.622601
240.982638	7345.197526	14.666202	-0.048862	4.620163
240.783681	7337.194083	14.671207	-0.048819	4.617722
240.873589	7329.212312	14.676211	-0.048831	4.615286
240.676631	7321.169402	14.681216	-0.048788	4.612830
240.801027	7313.147047	14.686221	-0.048806	4.610379
240.767876	7305.211729	14.691226	-0.048795	4.607953
240.685664	7297.124523	14.696231	-0.048774	4.605479
240.747110	7289.183316	14.701235	-0.048780	4.603049
240.651817	7281.173092	14.706240	-0.048757	4.600597
240.678848	7273.184326	14.711245	-0.048756	4.598149
240.672315	7265.219215	14.716250	-0.048750	4.595708
240.520988	7257.102902	14.721255	-0.048716	4.593219
240.546660	7249.128015	14.726259	-0.048716	4.590772
240.444035	7241.117000	14.731264	-0.048691	4.588312
240.421182	7233.083716	14.736269	-0.048681	4.585845
240.517868	7225.164140	14.741274	-0.048694	4.583411
240.549746	7217.167723	14.746279	-0.048695	4.580952
240.449506	7209.186139	14.751283	-0.048670	4.578496
240.386779	7201.130694	14.756288	-0.048653	4.576016
240.438873	7193.099525	14.761293	-0.048658	4.573543
240.362043	7185.151140	14.766298	-0.048638	4.571093
240.330172	7177.142098	14.771303	-0.048627	4.568624
240.447693	7169.153001	14.776307	-0.048643	4.566159
240.175886	7161.132392	14.781312	-0.048587	4.563683
240.224940	7153.161337	14.786317	-0.048591	4.561221
240.374926	7145.170884	14.791322	-0.048613	4.558752
240.019979	7137.116444	14.796327	-0.048542	4.556262
239.974453	7129.153813	14.801331	-0.048528	4.553798
240.061270	7121.127273	14.806336	-0.048539	4.551314
239.950766	7113.061797	14.811341	-0.048513	4.548816
239.836195	7105.132783	14.816346	-0.048486	4.546359
239.768927	7097.102128	14.821351	-0.048468	4.543870
239.898436	7089.146186	14.826355	-0.048487	4.541402
239.821365	7081.139472	14.831360	-0.048467	4.538917
239.828297	7073.129617	14.836365	-0.048463	4.536429
239.984690	7065.142276	14.841370	-0.048486	4.533948
239.897185	7057.092616	14.846375	-0.048465	4.531446
239.748575	7049.128141	14.851379	-0.048432	4.528968
239.644291	7041.074509	14.856384	-0.048407	4.526461
239.671420	7033.102614	14.861389	-0.048406	4.523979
239.680658	7025.182310	14.866394	-0.048403	4.521511
239.663789	7017.116350	14.871399	-0.048394	4.518997
239.627100	7009.159121	14.876403	-0.048382	4.516515
239.657738	7001.097734	14.881408	-0.048382	4.513999
239.635653	6992.987296	14.886413	-0.048373	4.511467
239.682063	6985.075657	14.891418	-0.048376	4.508995
239.530025	6977.050244	14.896423	-0.048342	4.506486
239.500549	6969.083172	14.901427	-0.048331	4.503994
239.487599	6961.072508	14.906432	-0.048324	4.501487
239.390260	6953.063111	14.911437	-0.048300	4.498979
239.182984	6945.101102	14.916442	-0.048256	4.496483
239.309808	6937.073688	14.921447	-0.048274	4.493967
239.251086	6929.056525	14.926451	-0.048258	4.491453
239.088799	6921.032983	14.931456	-0.048222	4.488934
239.043156	6913.066504	14.936461	-0.048208	4.486432
239.032169	6905.056452	14.941466	-0.048201	4.483916
239.247470	6897.057455	14.946471	-0.048235	4.481402
239.080716	6889.060034	14.951475	-0.048199	4.478886
239.023041	6881.125491	14.956480	-0.048183	4.476389
239.204416	6873.044066	14.961485	-0.048211	4.473845
239.132307	6865.049298	14.966490	-0.048192	4.471325
238.840640	6856.984380	14.971495	-0.048133	4.468782
238.911395	6849.040646	14.976499	-0.048140	4.466277
239.103656	6841.022765	14.981504	-0.048171	4.463747
238.908782	6833.027888	14.986509	-0.048129	4.461221
239.090404	6825.032992	14.991514	-0.048158	4.458696
239.040547	6817.050391	14.996519	-0.048143	4.456172
238.869414	6809.054145	15.001523	-0.048106	4.453642
238.672074	6801.030316	15.006528	-0.048063	4.451102
238.763135	6793.003439	15.011533	-0.048075	4.448560
238.866505	6785.038090	15.016538	-0.048089	4.446037
238.754206	6777.006301	15.021543	-0.048062	4.443490
238.802242	6769.056675	15.026547	-0.048066	4.440968
238.845717	6761.032951	15.031552	-0.048069	4.438421
238.687237	6753.021574	15.036557	-0.048034	4.435876
238.634578	6745.016306	15.041562	-0.048019	4.433332
238.801854	6736.958500	15.046567	-0.048044	4.430771
238.747963	6728.990938	15.051571	-0.048029	4.428236
238.543653	6720.967447	15.056576	-0.047985	4.425681
238.583438	6713.009688	15.061581	-0.047987	4.423146
238.382155	6705.034686	15.066586	-0.047944	4.420604
238.184776	6696.991871	15.071591	-0.047902	4.418038
238.471145	6689.003007	15.076595	-0.047950	4.415491
238.332461	6680.964746	15.081600	-0.047919	4.412924
238.189771	6672.955716	15.086605	-0.047887	4.410365
238.272804	6664.984855	15.091610	-0.047897	4.407817
238.280476	6656.972967	15.096615	-0.047893	4.405255
238.163192	6649.033164	15.101619	-0.047866	4.402714
238.100828	6641.016172	15.106624	-0.047849	4.400147
238.140917	6633.061583	15.111629	-0.047851	4.397598
238.073555	6625.005364	15.116634	-0.047833	4.395016
237.835686	6616.966603	15.121639	-0.047783	4.392436
238.150068	6608.953133	15.126643	-0.047836	4.389866
238.108441	6600.984569	15.131648	-0.047823	4.387307
237.958127	6592.990570	15.136653	-0.047790	4.384737
237.973116	6585.043959	15.141658	-0.047787	4.382183
237.877882	6576.972052	15.146663	-0.047764	4.379585
237.826098	6569.031199	15.151667	-0.047749	4.377029
237.763996	6560.969227	15.156672	-0.047732	4.374432
237.612253	6552.949603	15.161677	-0.047698	4.371847
238.067078	6544.967745	15.166682	-0.047778	4.369276
237.812232	6537.004088	15.171687	-0.047725	4.366705
237.710134	6528.991985	15.176691	-0.047700	4.364118
237.690384	6521.060360	15.181696	-0.047691	4.361556
237.803450	6512.974343	15.186701	-0.047707	4.358943
237.864286	6505.064999	15.191706	-0.047713	4.356385
237.583823	6496.950182	15.196711	-0.047655	4.353757
237.647547	6488.874800	15.201715	-0.047662	4.351143
237.609472	6480.901723	15.206720	-0.047649	4.348560
237.612673	6472.924846	15.211725	-0.047644	4.345974
237.611786	6464.985524	15.216730	-0.047639	4.343398
237.376730	6456.966457	15.221735	-0.047589	4.340794
237.571293	6449.009421	15.226739	-0.047620	4.338211
237.651282	6440.950038	15.231744	-0.047630	4.335593
237.455349	6432.965822	15.236749	-0.047588	4.332995
237.289410	6424.959921	15.241754	-0.047552	4.330389
237.506499	6416.929329	15.246759	-0.047587	4.327776
237.435656	6408.939650	15.251763	-0.047568	4.325173
237.249844	6401.012950	15.256768	-0.047528	4.322588
237.183639	6392.925668	15.261773	-0.047510	4.319950
237.258221	6385.011323	15.266778	-0.047519	4.317368
237.141606	6376.925467	15.271783	-0.047492	4.314727
237.078661	6368.924559	15.276787	-0.047474	4.312112
237.142760	6360.914093	15.281792	-0.047481	4.309494
237.182509	6352.899515	15.286797	-0.047483	4.306872
237.202334	6344.948448	15.291802	-0.047481	4.304270
236.970043	6336.977776	15.296807	-0.047433	4.301657
236.970486	6328.913064	15.301811	-0.047427	4.299014
236.937585	6320.966441	15.306816	-0.047416	4.296408
236.807420	6312.896756	15.311821	-0.047386	4.293759
237.161178	6304.920829	15.316826	-0.047447	4.291143
236.651890	6296.905726	15.321831	-0.047346	4.288505
236.639271	6288.927837	15.326835	-0.047339	4.285883
236.744271	6280.975569	15.331840	-0.047353	4.283268
236.746703	6272.918866	15.336845	-0.047348	4.280616
236.727136	6264.950175	15.341850	-0.047339	4.277991
236.594336	6256.944829	15.346855	-0.047309	4.275352
236.709484	6248.892552	15.351859	-0.047325	4.272697
236.526406	6240.910822	15.356864	-0.047285	4.270062
236.495837	6232.851582	15.361869	-0.047274	4.267401
236.697911	6224.896956	15.366874	-0.047306	4.264775
236.620390	6216.891454	15.371879	-0.047286	4.262128
236.575143	6208.916505	15.376883	-0.047272	4.259489
236.495499	6200.911635	15.381888	-0.047252	4.256839
236.425402	6192.918124	15.386893	-0.047234	4.254191
236.501317	6184.907676	15.391898	-0.047242	4.251537
236.273781	6176.903169	15.396903	-0.047195	4.248880
236.364492	6168.923959	15.401907	-0.047206	4.246233
236.488681	6160.953447	15.406912	-0.047224	4.243588
236.150964	6152.931539	15.411917	-0.047156	4.240920
236.190210	6144.970641	15.416922	-0.047158	4.238274
236.075696	6136.928151	15.421927	-0.047131	4.235597
236.049667	6128.964168	15.426931	-0.047121	4.232946
236.052936	6120.922812	15.431936	-0.047116	4.230267
236.070359	6112.932023	15.436941	-0.047114	4.227604
235.949954	6104.918548	15.441946	-0.047086	4.224931
235.981536	6096.969254	15.446951	-0.047086	4.222278
236.173762	6088.931320	15.451955	-0.047117	4.219596
236.127541	6080.980378	15.456960	-0.047103	4.216939
235.779746	6072.948456	15.461965	-0.047032	4.214250
235.903887	6064.953971	15.466970	-0.047050	4.211577
235.740070	6056.910949	15.471975	-0.047014	4.208882
235.645033	6048.947413	15.476979	-0.046991	4.206214
235.796088	6040.943108	15.481984	-0.047014	4.203532
235.821675	6032.932918	15.486989	-0.047013	4.200846
235.802754	6024.988771	15.491994	-0.047004	4.198179
235.730910	6016.933351	15.496999	-0.046985	4.195473
235.730458	6008.854876	15.502003	-0.046980	4.192758
235.591261	6000.858505	15.507008	-0.046949	4.190068
235.568090	5992.833892	15.512013	-0.046939	4.187367
235.776284	5984.882005	15.517018	-0.046972	4.184692
235.477241	5976.911014	15.522023	-0.046911	4.182003
235.433362	5968.897052	15.527027	-0.046898	4.179300
235.426373	5960.964783	15.532032	-0.046891	4.176624
235.490245	5952.899340	15.537037	-0.046897	4.173902
235.416858	5944.902881	15.542042	-0.046878	4.171200
235.241608	5936.907696	15.547047	-0.046840	4.168496
235.282680	5928.881827	15.552051	-0.046842	4.165781
235.191390	5920.925638	15.557056	-0.046820	4.163087
235.105856	5912.919158	15.562061	-0.046799	4.160375
235.262053	5904.935373	15.567066	-0.046822	4.157671
235.119890	5896.925682	15.572071	-0.046790	4.154953
235.272333	5888.899048	15.577075	-0.046813	4.152231
235.273126	5880.861812	15.582080	-0.046808	4.149501
235.117271	5872.856532	15.587085	-0.046774	4.146779
234.985257	5864.888776	15.592090	-0.046744	4.144068
234.976399	5856.936573	15.597095	-0.046737	4.141363
234.842114	5848.891417	15.602099	-0.046706	4.138622
234.931050	5840.948025	15.607104	-0.046717	4.135916
234.767137	5832.917363	15.612109	-0.046681	4.133177
235.072054	5824.875909	15.617114	-0.046733	4.130437
234.739984	5816.864869	15.622119	-0.046666	4.127698
234.757703	5808.886590	15.627123	-0.046663	4.124973
234.858604	5800.937891	15.632128	-0.046677	4.122257
234.757761	5792.911586	15.637133	-0.046653	4.119510
234.770643	5784.975781	15.642138	-0.046650	4.116794
234.619904	5776.893738	15.647143	-0.046616	4.114024
234.538756	5768.869211	15.652147	-0.046596	4.111273
234.600273	5760.900178	15.657152	-0.046602	4.108540
234.342890	5752.867688	15.662157	-0.046548	4.105780
234.516391	5744.917757	15.667162	-0.046575	4.103052
234.526947	5736.883080	15.672167	-0.046572	4.100291
234.327141	5728.950014	15.677171	-0.046529	4.097560
234.619986	5720.936904	15.682176	-0.046578	4.094807
234.427119	5712.870169	15.687181	-0.046537	4.092026
234.453090	5704.907255	15.692186	-0.046536	4.089283
234.250031	5696.937932	15.697191	-0.046493	4.086532
234.249443	5688.943400	15.702195	-0.046488	4.083773
234.368885	5680.959423	15.707200	-0.046505	4.081018
234.241919	5672.956370	15.712205	-0.046475	4.078251
234.129130	5664.967263	15.717210	-0.046449	4.075487
234.182911	5656.918244	15.722215	-0.046454	4.072703
234.408273	5648.896568	15.727219	-0.046490	4.069929
234.177481	5640.946693	15.732224	-0.046442	4.067171
233.995034	5632.896805	15.737229	-0.046402	4.064377
234.068489	5624.967896	15.742234	-0.046411	4.061627
234.035646	5616.944470	15.747239	-0.046399	4.058841
234.022844	5608.981435	15.752243	-0.046391	4.056075
234.158983	5600.957459	15.757248	-0.046411	4.053287
233.962493	5592.892853	15.762253	-0.046369	4.050479
234.059335	5584.936271	15.767258	-0.046382	4.047710
234.055689	5576.909639	15.772263	-0.046376	4.044914
233.908235	5568.996761	15.777267	-0.046343	4.042153
233.867494	5560.962221	15.782272	-0.046330	4.039349
233.768414	5552.985859	15.787277	-0.046306	4.036563
233.899419	5544.931844	15.792282	-0.046325	4.033751
233.802997	5536.832575	15.797287	-0.046302	4.030919
233.544062	5528.869252	15.802291	-0.046248	4.028129
233.539325	5520.870106	15.807296	-0.046242	4.025328
233.454642	5512.927272	15.812301	-0.046221	4.022544
233.736544	5504.919462	15.817306	-0.046268	4.019741
233.663330	5496.918668	15.822311	-0.046249	4.016934
233.410377	5488.915523	15.827315	-0.046196	4.014120
233.259833	5480.934836	15.832320	-0.046163	4.011314
233.431599	5472.889370	15.837325	-0.046189	4.008488
233.494297	5464.927187	15.842330	-0.046196	4.005688
233.215523	5456.943500	15.847335	-0.046138	4.002873
233.193924	5448.941428	15.852339	-0.046129	4.000053
233.287606	5440.974263	15.857344	-0.046141	3.997246
233.339700	5432.890728	15.862349	-0.046145	3.994395
233.265693	5424.929270	15.867354	-0.046126	3.991583
233.181819	5416.905015	15.872359	-0.046105	3.988747
233.233029	5408.894347	15.877363	-0.046109	3.985915
233.277838	5400.931115	15.882368	-0.046112	3.983099
233.103049	5392.908886	15.887373	-0.046074	3.980256
233.305030	5384.950466	15.892378	-0.046106	3.977439
233.174670	5376.936753	15.897383	-0.046077	3.974596
233.101954	5368.950728	15.902387	-0.046058	3.971761
233.203449	5360.959493	15.907392	-0.046071	3.968925
233.181509	5352.949984	15.912397	-0.046062	3.966079
233.063299	5344.975448	15.917402	-0.046034	3.963241
232.993104	5336.972787	15.922407	-0.046016	3.960392
232.838263	5329.007194	15.927411	-0.045981	3.957553
232.858658	5321.005580	15.932416	-0.045980	3.954702
232.749189	5312.936443	15.937421	-0.045954	3.951823
232.828738	5304.965410	15.942426	-0.045963	3.948980
232.773456	5296.968283	15.947431	-0.045948	3.946123
232.696679	5288.982407	15.952435	-0.045928	3.943267
232.824257	5281.001809	15.957440	-0.045946	3.940415
232.772652	5273.009713	15.962445	-0.045931	3.937554
232.696458	5265.014229	15.967450	-0.045912	3.934689
232.688643	5256.966319	15.972455	-0.045905	3.931804
232.639022	5248.998650	15.977459	-0.045890	3.928945
232.498176	5241.009256	15.982464	-0.045859	3.926075
232.456885	5232.989438	15.987469	-0.045846	3.923194
232.560373	5224.997671	15.992474	-0.045859	3.920323
232.517399	5217.032233	15.997479	-0.045846	3.917456
232.282466	5209.022697	16.002483	-0.045797	3.914568
232.398005	5201.001104	16.007488	-0.045813	3.911681
232.334760	5192.951368	16.012493	-0.045796	3.908777
232.347911	5185.013528	16.017498	-0.045793	3.905913
232.344961	5177.020119	16.022503	-0.045787	3.903027
232.355865	5168.975767	16.027507	-0.045783	3.900120
232.183576	5161.054920	16.032512	-0.045746	3.897253
231.990888	5152.997039	16.037517	-0.045705	3.894333
232.311858	5145.002553	16.042522	-0.045759	3.891444
232.253455	5136.984085	16.047527	-0.045743	3.888537
232.029931	5128.993356	16.052531	-0.045696	3.885634
232.018571	5121.030020	16.057536	-0.045688	3.882744
231.765222	5113.020326	16.062541	-0.045636	3.879829
231.902835	5105.061799	16.067546	-0.045656	3.876939
231.812229	5096.955073	16.072551	-0.045633	3.873988
232.150019	5088.750735	16.077555	-0.045691	3.871008
231.980774	5080.888565	16.082560	-0.045654	3.868140
231.743387	5072.906783	16.087565	-0.045604	3.865225
231.834165	5064.983260	16.092570	-0.045616	3.862335
231.906361	5056.987176	16.097575	-0.045624	3.859417
231.749486	5049.019167	16.102579	-0.045589	3.856502
231.598516	5041.033036	16.107584	-0.045556	3.853578
231.513071	5032.978619	16.112589	-0.045534	3.850628
231.615140	5024.988111	16.117594	-0.045548	3.847704
231.621398	5016.983468	16.122599	-0.045544	3.844770
231.611063	5009.026708	16.127603	-0.045537	3.841851
231.363258	5001.102153	16.132608	-0.045485	3.838936
231.211763	4993.078895	16.137613	-0.045451	3.835985
231.474706	4985.061261	16.142618	-0.045495	3.833043
231.352985	4977.034282	16.147623	-0.045467	3.830087
231.220252	4969.017581	16.152627	-0.045437	3.827132
231.487411	4961.007900	16.157632	-0.045481	3.824185
231.470988	4953.068842	16.162637	-0.045473	3.821257
231.410296	4945.113075	16.167642	-0.045456	3.818319
231.131038	4937.117836	16.172647	-0.045399	3.815360
231.244443	4929.062197	16.177651	-0.045414	3.812384
231.315821	4921.082741	16.182656	-0.045422	3.809434
231.087713	4913.062072	16.187661	-0.045374	3.806459
231.228746	4905.106951	16.192666	-0.045395	3.803514
231.153752	4897.090718	16.197671	-0.045376	3.800540
231.045918	4889.138241	16.202675	-0.045350	3.797586
231.085518	4881.121081	16.207680	-0.045352	3.794609
230.856802	4873.049767	16.212685	-0.045304	3.791604
231.089194	4865.063135	16.217690	-0.045342	3.788638
231.027063	4857.069286	16.222695	-0.045325	3.785661
231.054096	4849.102369	16.227699	-0.045325	3.782693
231.040788	4841.111490	16.232704	-0.045317	3.779713
230.503755	4833.126818	16.237709	-0.045211	3.776721
230.634903	4825.106507	16.242714	-0.045230	3.773729
230.654579	4817.093447	16.247719	-0.045229	3.770734
230.653874	4809.079652	16.252723	-0.045223	3.767737
230.629768	4801.097851	16.257728	-0.045213	3.764748
230.601071	4793.110193	16.262733	-0.045202	3.761754
230.626850	4785.149691	16.267738	-0.045202	3.758770
230.458968	4777.145108	16.272743	-0.045165	3.755762
230.548244	4769.119436	16.277747	-0.045176	3.752750
230.641172	4761.098288	16.282752	-0.045188	3.749738
230.304438	4753.064737	16.287757	-0.045120	3.746708
230.376076	4745.115892	16.292762	-0.045128	3.743717
230.515918	4737.141760	16.297767	-0.045149	3.740716
230.382151	4729.143204	16.302771	-0.045118	3.737696
230.170763	4721.151119	16.307776	-0.045074	3.734675
230.236128	4713.160456	16.312781	-0.045080	3.731659
230.227504	4705.126447	16.317786	-0.045073	3.728622
230.090271	4697.122867	16.322791	-0.045042	3.725590
230.130366	4689.159037	16.327795	-0.045044	3.722576
230.154342	4681.174678	16.332800	-0.045044	3.719551
230.199772	4673.213535	16.337805	-0.045047	3.716533
230.264119	4665.162245	16.342810	-0.045053	3.713479
230.199200	4657.074166	16.347815	-0.045036	3.710405
230.016469	4649.105545	16.352819	-0.044996	3.707371
229.989946	4641.155509	16.357824	-0.044986	3.704345
229.888535	4633.179178	16.362829	-0.044962	3.701306
229.878528	4625.203464	16.367834	-0.044954	3.698266
229.589296	4617.206025	16.372839	-0.044895	3.695208
229.804178	4609.229543	16.377843	-0.044930	3.692168
229.844290	4601.231064	16.382848	-0.044932	3.689114
229.644671	4593.199590	16.387853	-0.044889	3.686037
229.588159	4585.239609	16.392858	-0.044873	3.682990
229.510693	4577.241204	16.397863	-0.044853	3.679924
229.656546	4569.271210	16.402867	-0.044875	3.676873
229.572309	4561.245924	16.407872	-0.044854	3.673792
229.534459	4553.216169	16.412877	-0.044842	3.670707
229.529503	4545.256745	16.417882	-0.044835	3.667649
229.504005	4537.216107	16.422887	-0.044825	3.664555
229.583368	4529.252992	16.427891	-0.044834	3.661492
229.578982	4521.265757	16.432896	-0.044828	3.658415
229.166826	4513.291209	16.437901	-0.044746	3.655329
229.307693	4505.271206	16.442906	-0.044767	3.652237
229.624535	4497.206278	16.447911	-0.044820	3.649131
229.261724	4489.257797	16.452915	-0.044748	3.646048
229.071669	4481.278480	16.457920	-0.044707	3.642956
228.978286	4473.238900	16.462925	-0.044684	3.639840
229.417016	4465.304618	16.467930	-0.044760	3.636777
229.252172	4457.300549	16.472935	-0.044724	3.633668
229.116865	4449.255533	16.477939	-0.044693	3.630541
229.222096	4441.274579	16.482944	-0.044708	3.627442
228.852575	4433.259875	16.487949	-0.044633	3.624315
228.850573	4425.325028	16.492954	-0.044628	3.621227
228.718127	4417.308427	16.497959	-0.044598	3.618100
228.707490	4409.318221	16.502963	-0.044590	3.614984
228.669347	4401.334466	16.507968	-0.044578	3.611868
228.761102	4393.266894	16.512973	-0.044589	3.608719
228.780890	4385.304059	16.517978	-0.044588	3.605607
228.784998	4377.352408	16.522983	-0.044583	3.602496
228.733134	4369.351875	16.527987	-0.044568	3.599361
228.784573	4361.410632	16.532992	-0.044572	3.596250
228.645903	4353.368231	16.537997	-0.044541	3.593091
228.409058	4345.403649	16.543002	-0.044491	3.589957
228.507165	4337.377397	16.548007	-0.044504	3.586806
228.625585	4329.386041	16.553011	-0.044521	3.583666
228.484558	4321.411027	16.558016	-0.044489	3.580523
228.368874	4313.403218	16.563021	-0.044462	3.577364
228.535142	4305.408799	16.568026	-0.044488	3.574216
228.325732	4297.416520	16.573031	-0.044443	3.571056
228.134568	4289.424546	16.578035	-0.044402	3.567893
228.306524	4281.399534	16.583040	-0.044429	3.564725
228.355341	4273.436430	16.588045	-0.044433	3.561574
228.346574	4265.431845	16.593050	-0.044426	3.558403
228.412487	4257.453250	16.598055	-0.044433	3.555242
228.248446	4249.358113	16.603059	-0.044397	3.552025
228.311867	4241.387734	16.608064	-0.044403	3.548861
228.047394	4233.371308	16.613069	-0.044348	3.545666
228.080172	4225.428514	16.618074	-0.044349	3.542507
228.223016	4217.412416	16.623079	-0.044370	3.539319
228.080563	4209.455566	16.628083	-0.044338	3.536143
228.118071	4201.471187	16.633088	-0.044340	3.532958
227.861585	4193.459273	16.638093	-0.044287	3.529751
227.859098	4185.472122	16.643098	-0.044281	3.526558
227.878174	4177.469506	16.648103	-0.044279	3.523357
227.889312	4169.477883	16.653107	-0.044276	3.520158
227.767924	4161.550410	16.658112	-0.044248	3.516977
227.556113	4153.514215	16.663117	-0.044203	3.513746
227.704905	4145.498127	16.668122	-0.044225	3.510532
227.784462	4137.494669	16.673127	-0.044235	3.507318
227.485561	4129.527838	16.678131	-0.044173	3.504104
227.696052	4121.556022	16.683136	-0.044207	3.500901
227.770567	4113.552442	16.688141	-0.044216	3.497678
227.698181	4105.546789	16.693146	-0.044197	3.494446
227.452670	4097.562128	16.698151	-0.044146	3.491214
227.265974	4089.573416	16.703155	-0.044106	3.487980
227.468006	4081.593266	16.708160	-0.044138	3.484758
227.219435	4073.618163	16.713165	-0.044086	3.481522
227.566409	4065.596606	16.718170	-0.044145	3.478282
227.419278	4057.617662	16.723175	-0.044112	3.475041
226.980398	4049.602537	16.728179	-0.044025	3.471772
227.055872	4041.601832	16.733184	-0.044034	3.468523
227.260022	4033.563037	16.738189	-0.044067	3.465260
227.061493	4025.620652	16.743194	-0.044024	3.462019
226.970165	4017.622839	16.748199	-0.044002	3.458757
226.978615	4009.628426	16.753203	-0.043998	3.455496
226.877168	4001.651179	16.758208	-0.043974	3.452235
226.731459	3993.610271	16.763213	-0.043941	3.448944
226.751340	3985.650664	16.768218	-0.043939	3.445688
226.755059	3977.667881	16.773223	-0.043935	3.442420
226.717174	3969.663331	16.778227	-0.043922	3.439138
226.694375	3961.689554	16.783232	-0.043913	3.435865
226.785317	3953.666981	16.788237	-0.043924	3.432574
226.729727	3945.645851	16.793242	-0.043908	3.429275
226.649525	3937.691373	16.798247	-0.043888	3.425999
226.660027	3929.679495	16.803251	-0.043885	3.422700
226.805389	3921.722503	16.808256	-0.043906	3.419425
226.633237	3913.740342	16.813261	-0.043869	3.416125
226.607940	3905.735675	16.818266	-0.043859	3.412818
226.622329	3897.709825	16.823271	-0.043856	3.409500
226.368248	3889.763154	16.828275	-0.043803	3.406203
226.274833	3881.815411	16.833280	-0.043780	3.402907
226.232908	3873.774781	16.838285	-0.043767	3.399572
226.405400	3865.813555	16.843290	-0.043794	3.396273
226.218616	3857.767756	16.848295	-0.043754	3.392924
226.254836	3849.690950	16.853299	-0.043755	3.389566
226.162793	3841.773889	16.858304	-0.043733	3.386267
226.064809	3833.791705	16.863309	-0.043709	3.382937
226.086752	3825.800526	16.868314	-0.043708	3.379605
226.319376	3817.848641	16.873319	-0.043746	3.376293
225.985699	3809.821294	16.878323	-0.043678	3.372926
226.086411	3801.806800	16.883328	-0.043691	3.369577
225.862566	3793.863034	16.888333	-0.043644	3.366243
225.900888	3785.866794	16.893338	-0.043646	3.362892
225.758674	3777.879159	16.898343	-0.043614	3.359535
225.576659	3769.919353	16.903347	-0.043575	3.356185
225.966909	3761.891445	16.908352	-0.043642	3.352824
225.663515	3753.864717	16.913357	-0.043580	3.349435
225.714588	3745.893284	16.918362	-0.043584	3.346078
225.736715	3737.913109	16.923367	-0.043583	3.342714
225.709534	3729.896472	16.928371	-0.043572	3.339329
225.794253	3721.952793	16.933376	-0.043583	3.335975
225.713042	3713.916509	16.938381	-0.043562	3.332573
225.712474	3705.916037	16.943386	-0.043557	3.329185
225.461192	3697.974465	16.948391	-0.043505	3.325810
225.539499	3689.961298	16.953395	-0.043514	3.322412
225.709086	3681.976887	16.958400	-0.043540	3.319028
225.466419	3674.021610	16.963405	-0.043489	3.315636
225.516192	3666.013468	16.968410	-0.043493	3.312230
225.700710	3657.981063	16.973415	-0.043522	3.308815
225.489483	3649.991382	16.978419	-0.043477	3.305399
225.529697	3642.053404	16.983424	-0.043480	3.302012
225.348494	3634.037489	16.988429	-0.043440	3.298579
225.528392	3626.052345	16.993434	-0.043468	3.295170
225.406132	3618.052251	16.998439	-0.043440	3.291739
225.241655	3610.070185	17.003443	-0.043404	3.288311
225.248214	3602.088367	17.008448	-0.043400	3.284886
225.226540	3594.096363	17.013453	-0.043391	3.281451
225.242897	3586.110746	17.018458	-0.043388	3.278018
225.026319	3578.134348	17.023463	-0.043343	3.274576
225.015231	3570.126750	17.028467	-0.043335	3.271124
224.791546	3562.163636	17.033472	-0.043288	3.267680
224.938500	3554.107242	17.038477	-0.043310	3.264206
224.889965	3546.158817	17.043482	-0.043296	3.260768
224.873620	3538.186289	17.048487	-0.043287	3.257317
224.816673	3530.156094	17.053491	-0.043271	3.253836
225.004193	3522.137896	17.058496	-0.043301	3.250366
224.909072	3514.175837	17.063501	-0.043277	3.246905
224.863139	3506.191202	17.068506	-0.043264	3.243433
224.811358	3498.234332	17.073511	-0.043249	3.239968
224.689212	3490.265317	17.078515	-0.043220	3.236492
224.656412	3482.252240	17.083520	-0.043209	3.232997
224.431647	3474.215725	17.088525	-0.043162	3.229480
224.640536	3466.218933	17.093530	-0.043195	3.225994
224.410147	3458.254729	17.098535	-0.043147	3.222500
224.274770	3450.256157	17.103539	-0.043116	3.218992
224.431953	3442.278707	17.108544	-0.043140	3.215501
224.256201	3434.303556	17.113549	-0.043102	3.211993
224.292568	3426.304384	17.118554	-0.043103	3.208480
224.426783	3418.291219	17.123559	-0.043123	3.204961
224.366841	3410.330720	17.128563	-0.043106	3.201453
224.476098	3402.374930	17.133568	-0.043121	3.197950
224.363598	3394.352061	17.138573	-0.043095	3.194405
224.191436	3386.376341	17.143578	-0.043057	3.190874
224.059265	3378.408535	17.148583	-0.043027	3.187344
223.883002	3370.399588	17.153587	-0.042989	3.183791
224.108237	3362.410397	17.158592	-0.043026	3.180259
224.083397	3354.428721	17.163597	-0.043016	3.176715
223.927035	3346.456003	17.168602	-0.042981	3.173167
223.908942	3338.429119	17.173607	-0.042972	3.169596
223.978025	3330.454011	17.178611	-0.042980	3.166048
223.882009	3322.493325	17.183616	-0.042957	3.162495
223.715031	3314.503784	17.188621	-0.042920	3.158922
223.986834	3306.499502	17.193626	-0.042965	3.155358
223.801523	3298.497107	17.198631	-0.042925	3.151770
223.639754	3290.486289	17.203635	-0.042890	3.148176
223.892805	3282.487922	17.208640	-0.042932	3.144601
223.701455	3274.560215	17.213645	-0.042891	3.141034
223.731198	3266.552513	17.218650	-0.042891	3.137438
223.646748	3258.595752	17.223655	-0.042870	3.133854
223.765571	3250.549090	17.228659	-0.042886	3.130236
223.549437	3242.632692	17.233664	-0.042841	3.126657
223.289998	3234.622623	17.238669	-0.042787	3.123029
223.380755	3226.649358	17.243674	-0.042798	3.119430
223.227102	3218.699914	17.248679	-0.042764	3.115826
223.119878	3210.662819	17.253683	-0.042739	3.112181
223.138792	3202.665257	17.258688	-0.042737	3.108554
223.228419	3194.647953	17.263693	-0.042748	3.104918
223.187511	3186.705940	17.268698	-0.042735	3.101306
223.173035	3178.738325	17.273703	-0.042727	3.097679
223.217408	3170.715922	17.278707	-0.042730	3.094026
223.281260	3162.716058	17.283712	-0.042737	3.090379
223.258920	3154.719969	17.288717	-0.042727	3.086726
223.259860	3146.760345	17.293722	-0.042722	3.083087
223.325815	3138.776949	17.298727	-0.042729	3.079435
222.909477	3130.848594	17.303731	-0.042646	3.075781
222.984629	3122.767650	17.308736	-0.042654	3.072077
223.029511	3114.742290	17.313741	-0.042657	3.068391
222.984679	3106.772347	17.318746	-0.042644	3.064723
222.932123	3098.857476	17.323751	-0.042628	3.061075
222.858223	3090.868998	17.328755	-0.042609	3.057388
222.907898	3082.881553	17.333760	-0.042613	3.053703
222.669010	3074.879437	17.338765	-0.042563	3.049993
222.573078	3066.909516	17.343770	-0.042540	3.046300
222.504867	3058.953854	17.348775	-0.042522	3.042610
222.335689	3050.956459	17.353779	-0.042485	3.038892
222.462961	3042.977149	17.358784	-0.042503	3.035192
222.389646	3034.990112	17.363789	-0.042484	3.031474
222.416491	3026.979702	17.368794	-0.042484	3.027745
222.321609	3019.016608	17.373799	-0.042461	3.024028
222.396901	3011.008141	17.378803	-0.042469	3.020293
222.514013	3003.057236	17.383808	-0.042486	3.016583
222.375474	2995.044854	17.388813	-0.042455	3.012827
222.200271	2987.051053	17.393818	-0.042417	3.009073
222.198421	2979.080330	17.398823	-0.042411	3.005334
221.957439	2971.130136	17.403827	-0.042361	3.001588
222.115418	2963.138551	17.408832	-0.042385	2.997837
222.132243	2955.135386	17.413837	-0.042382	2.994070
222.167793	2947.096624	17.418842	-0.042383	2.990282
222.103311	2939.160617	17.423847	-0.042366	2.986532
222.065447	2931.149925	17.428851	-0.042354	2.982744
222.182368	2923.186328	17.433856	-0.042370	2.978981
222.125758	2915.213082	17.438861	-0.042354	2.975200
222.198086	2907.209243	17.443866	-0.042362	2.971406
222.016999	2899.238818	17.448871	-0.042323	2.967610
221.775964	2891.266103	17.453875	-0.042273	2.963805
221.683052	2883.331707	17.458880	-0.042250	2.960022
222.044967	2875.323157	17.463885	-0.042312	2.956221
221.824969	2867.347040	17.468890	-0.042266	2.952401
221.674317	2859.363422	17.473895	-0.042232	2.948576
221.488570	2851.362116	17.478899	-0.042192	2.944735
221.759392	2843.383613	17.483904	-0.042237	2.940925
221.470474	2835.416382	17.488909	-0.042178	2.937085
221.474043	2827.435649	17.493914	-0.042173	2.933249
221.673008	2819.392168	17.498919	-0.042205	2.929389
221.430296	2811.419774	17.503923	-0.042154	2.925534
221.595316	2803.486427	17.508928	-0.042180	2.921715
221.316903	2795.522906	17.513933	-0.042123	2.917852
221.349576	2787.516545	17.518938	-0.042123	2.913980
221.282180	2779.473866	17.523943	-0.042105	2.910080
221.232462	2771.470283	17.528947	-0.042091	2.906195
221.406968	2763.543862	17.533952	-0.042118	2.902354
221.351253	2755.558391	17.538957	-0.042102	2.898467
221.166773	2747.610109	17.543962	-0.042062	2.894585
221.458798	2739.588322	17.548967	-0.042111	2.890689
221.268084	2731.595127	17.553971	-0.042070	2.886775
221.135745	2723.663787	17.558976	-0.042040	2.882889
221.200054	2715.683033	17.563981	-0.042047	2.878984
221.024162	2707.725302	17.568986	-0.042009	2.875072
220.830670	2699.735992	17.573991	-0.041967	2.871138
220.641836	2691.755945	17.578995	-0.041927	2.867204
220.882160	2683.755819	17.584000	-0.041966	2.863278
220.760394	2675.771875	17.589005	-0.041938	2.859335
220.608047	2667.842270	17.594010	-0.041904	2.855411
220.747894	2659.810494	17.599015	-0.041925	2.851448
220.480971	2651.850342	17.604019	-0.041870	2.847492
220.505804	2643.868321	17.609024	-0.041869	2.843535
220.565141	2635.882165	17.614029	-0.041875	2.839573
220.561916	2627.933693	17.619034	-0.041869	2.835621
220.675391	2619.910318	17.624039	-0.041884	2.831633
220.700997	2611.909468	17.629043	-0.041884	2.827645
220.551941	2603.949233	17.634048	-0.041850	2.823662
220.457778	2595.982794	17.639053	-0.041828	2.819674
220.566883	2588.014328	17.644058	-0.041842	2.815690
220.636401	2580.019942	17.649063	-0.041850	2.811685
220.476830	2572.028485	17.654067	-0.041815	2.807663
220.083264	2564.117114	17.659072	-0.041736	2.803662
220.164811	2556.106624	17.664077	-0.041746	2.799633
220.197657	2548.133050	17.669082	-0.041747	2.795613
220.142442	2540.169393	17.674087	-0.041731	2.791588
219.852563	2532.184657	17.679091	-0.041672	2.787533
220.022773	2524.205635	17.684096	-0.041698	2.783501
219.926729	2516.226648	17.689101	-0.041675	2.779448
219.836459	2508.270962	17.694106	-0.041653	2.775402
220.004700	2500.259315	17.699111	-0.041678	2.771336
220.019091	2492.258967	17.704115	-0.041676	2.767261
219.885822	2484.331729	17.709120	-0.041646	2.763208
219.720648	2476.369266	17.714125	-0.041609	2.759129
219.803982	2468.383343	17.719130	-0.041619	2.755048
219.637992	2460.328401	17.724135	-0.041583	2.750910
219.511800	2452.351482	17.729139	-0.041554	2.746808
219.701949	2444.383145	17.734144	-0.041584	2.742723
219.630559	2436.422385	17.739149	-0.041566	2.738620
219.392446	2428.457058	17.744154	-0.041516	2.734499
219.429995	2420.475966	17.749159	-0.041517	2.730380
219.253719	2412.515440	17.754163	-0.041479	2.726253
219.137851	2404.582760	17.759168	-0.041452	2.722137
219.275841	2396.576513	17.764173	-0.041473	2.717992
219.217877	2388.601018	17.769178	-0.041456	2.713845
219.331975	2380.579370	17.774183	-0.041472	2.709679
219.117613	2372.647100	17.779187	-0.041427	2.705532
219.103974	2364.691047	17.784192	-0.041419	2.701379
218.985178	2356.734225	17.789197	-0.041392	2.697212
218.878406	2348.766266	17.794202	-0.041366	2.693034
218.944601	2340.770817	17.799207	-0.041373	2.688846
219.170228	2332.744751	17.804211	-0.041410	2.684645
218.836701	2324.865246	17.809216	-0.041342	2.680479
218.754232	2316.888973	17.814221	-0.041322	2.676272
218.960322	2308.849441	17.819226	-0.041354	2.672043
219.051326	2300.865441	17.824231	-0.041366	2.667830
218.786495	2292.913785	17.829235	-0.041311	2.663604
218.549722	2284.966179	17.834240	-0.041262	2.659375
218.662515	2276.988030	17.839245	-0.041277	2.655146
218.632102	2268.981403	17.844250	-0.041266	2.650886
218.497547	2261.051087	17.849255	-0.041236	2.646653
218.435214	2253.069999	17.854259	-0.041219	2.642390
218.651211	2245.100857	17.859264	-0.041254	2.638145
218.508990	2237.126188	17.864269	-0.041222	2.633867
218.423850	2229.141803	17.869274	-0.041201	2.629581
218.414495	2221.182030	17.874279	-0.041194	2.625306
218.196731	2213.229995	17.879283	-0.041148	2.621014
218.387285	2205.246860	17.884288	-0.041178	2.616725
218.470392	2197.243507	17.889293	-0.041188	2.612411
218.124878	2189.285848	17.894298	-0.041118	2.608086
218.174151	2181.334476	17.899303	-0.041122	2.603784
217.982291	2173.384305	17.904307	-0.041081	2.599459
218.045754	2165.431941	17.909312	-0.041087	2.595143
217.910665	2157.272270	17.914317	-0.041057	2.590694
217.896127	2149.299853	17.919322	-0.041048	2.586347
217.947135	2141.388031	17.924327	-0.041053	2.582030
217.775920	2133.452609	17.929331	-0.041015	2.577678
217.784485	2125.484994	17.934336	-0.041012	2.573313
217.987294	2117.492469	17.939341	-0.041044	2.568941
217.869889	2109.538544	17.944346	-0.041017	2.564560
217.741645	2101.646378	17.949351	-0.040987	2.560205
217.578246	2093.674621	17.954355	-0.040952	2.555796
217.708759	2085.678582	17.959360	-0.040970	2.551387
217.625156	2077.711652	17.964365	-0.040950	2.546971
217.690489	2069.734008	17.969370	-0.040956	2.542552
217.575590	2061.809162	17.974375	-0.040930	2.538142
217.407937	2053.828929	17.979379	-0.040893	2.533689
217.522519	2045.848568	17.984384	-0.040909	2.529249
217.508920	2037.881240	17.989389	-0.040901	2.524799
217.194342	2029.969614	17.994394	-0.040837	2.520351
217.231987	2022.017178	17.999399	-0.040839	2.515897
217.085811	2014.001305	18.004403	-0.040806	2.511387
217.381922	2005.983447	18.009408	-0.040856	2.506899
217.249532	1998.044437	18.014413	-0.040826	2.502417
217.166083	1990.097102	18.019418	-0.040805	2.497925
217.227578	1982.130739	18.024423	-0.040811	2.493425
217.108167	1974.166081	18.029427	-0.040783	2.488905
216.907263	1966.232306	18.034432	-0.040740	2.484388
216.993892	1958.263099	18.039437	-0.040751	2.479863
216.881257	1950.297612	18.044442	-0.040725	2.475318
216.875518	1942.333708	18.049447	-0.040718	2.470774
217.029257	1934.322446	18.054451	-0.040742	2.466205
217.008017	1926.393726	18.059456	-0.040732	2.461663
216.889882	1918.438786	18.064461	-0.040705	2.457090
216.619352	1910.502423	18.069466	-0.040649	2.452507
216.858880	1902.501639	18.074471	-0.040688	2.447917
216.726255	1894.551389	18.079475	-0.040658	2.443320
216.666811	1886.620571	18.084480	-0.040642	2.438730
216.484185	1878.659294	18.089485	-0.040602	2.434105
216.445855	1870.605786	18.094490	-0.040590	2.429429
216.472069	1862.667094	18.099495	-0.040589	2.424815
216.431759	1854.715084	18.104499	-0.040576	2.420180
216.407975	1846.772127	18.109504	-0.040567	2.415542
216.192068	1838.817146	18.114509	-0.040521	2.410873
216.031270	1830.850945	18.119514	-0.040486	2.406193
216.140127	1822.915688	18.124519	-0.040501	2.401543
216.045166	1814.952915	18.129523	-0.040478	2.396852
216.108015	1806.988936	18.134528	-0.040484	2.392164
215.850734	1799.043208	18.139533	-0.040431	2.387451
216.064049	1791.054231	18.144538	-0.040465	2.382741
216.084910	1783.114090	18.149543	-0.040463	2.378036
215.968281	1775.148260	18.154547	-0.040436	2.373294
215.832828	1767.197281	18.159552	-0.040406	2.368551
215.800494	1759.242138	18.164557	-0.040394	2.363804
215.798669	1751.301481	18.169562	-0.040389	2.359058
215.918883	1743.343896	18.174567	-0.040406	2.354303
215.641930	1735.356248	18.179571	-0.040349	2.349487
215.573572	1727.405121	18.184576	-0.040331	2.344701
215.598857	1719.469723	18.189581	-0.040330	2.339922
215.592592	1711.510112	18.194586	-0.040323	2.335116
215.605869	1703.539992	18.199591	-0.040320	2.330295
215.340584	1695.605788	18.204595	-0.040266	2.325463
215.438507	1687.643550	18.209600	-0.040278	2.320634
215.374121	1679.721529	18.214605	-0.040261	2.315806
215.200584	1671.753289	18.219610	-0.040223	2.310931
215.335561	1663.780607	18.224615	-0.040243	2.306068
215.043664	1655.855987	18.229619	-0.040183	2.301189
215.093721	1647.905175	18.234624	-0.040187	2.296312
214.994397	1639.954003	18.239629	-0.040164	2.291412
214.934820	1631.986598	18.244634	-0.040147	2.286494
214.991513	1624.048579	18.249639	-0.040152	2.281594
214.883730	1616.107484	18.254643	-0.040127	2.276668
214.926782	1608.081100	18.259648	-0.040129	2.271690
214.891302	1600.115240	18.264653	-0.040117	2.266733
214.687392	1592.190694	18.269658	-0.040074	2.261776
214.962804	1584.229517	18.274663	-0.040120	2.256827
214.873092	1576.275389	18.279667	-0.040098	2.251840
214.753921	1568.343285	18.284672	-0.040070	2.246852
214.514725	1560.429246	18.289677	-0.040020	2.241855
214.664611	1552.467256	18.294682	-0.040043	2.236850
214.719711	1544.520185	18.299687	-0.040048	2.231835
214.504512	1536.572641	18.304691	-0.040002	2.226785
214.420471	1528.648453	18.309696	-0.039981	2.221749
214.392383	1520.711365	18.314701	-0.039971	2.216699
214.345066	1512.736611	18.319706	-0.039957	2.211612
214.264841	1504.811465	18.324711	-0.039936	2.206541
214.252466	1496.857506	18.329715	-0.039929	2.201447
213.942525	1488.960833	18.334720	-0.039866	2.196350
213.942868	1480.984753	18.339725	-0.039860	2.191219
214.041144	1472.992674	18.344730	-0.039873	2.186074
214.232229	1465.041134	18.349735	-0.039903	2.180952
214.029637	1457.125535	18.354739	-0.039860	2.175805
214.012066	1449.173911	18.359744	-0.039852	2.170639
214.197782	1441.225670	18.364749	-0.039881	2.165482
213.823767	1433.327296	18.369754	-0.039806	2.160294
214.067861	1425.384433	18.374759	-0.039846	2.155121
213.951732	1417.428969	18.379763	-0.039819	2.149894
213.789376	1409.499777	18.384768	-0.039783	2.144667
213.737198	1401.573982	18.389773	-0.039768	2.139440
213.595811	1393.641910	18.394778	-0.039736	2.134187
213.696422	1385.682417	18.399783	-0.039750	2.128926
213.588613	1377.752779	18.404787	-0.039724	2.123652
213.453872	1369.852874	18.409792	-0.039694	2.118383
213.654552	1361.865864	18.414797	-0.039726	2.113074
213.324109	1353.906287	18.419802	-0.039659	2.107719
213.310179	1345.969956	18.424807	-0.039651	2.102396
213.417185	1338.035957	18.429811	-0.039666	2.097073
213.505018	1330.089387	18.434816	-0.039677	2.091727
213.240673	1322.186068	18.439821	-0.039622	2.086361
213.329401	1314.242223	18.444826	-0.039633	2.080989
213.229019	1306.346124	18.449831	-0.039609	2.075617
212.924324	1298.425457	18.454835	-0.039547	2.070193
212.870417	1290.484786	18.459840	-0.039532	2.064767
213.018552	1282.540242	18.464845	-0.039554	2.059344
213.030193	1274.595818	18.469850	-0.039551	2.053893
212.946194	1266.678547	18.474855	-0.039530	2.048436
212.810148	1258.754809	18.479859	-0.039499	2.042955
212.678637	1250.852877	18.484864	-0.039469	2.037475
212.539612	1242.919679	18.489869	-0.039438	2.031958
212.533584	1234.956011	18.494874	-0.039431	2.026418
212.732810	1227.013980	18.499879	-0.039463	2.020899
212.387421	1219.129149	18.504883	-0.039393	2.015349
212.388367	1211.194144	18.509888	-0.039388	2.009784
212.514738	1203.251422	18.514893	-0.039406	2.004211
212.198750	1195.372203	18.519898	-0.039342	1.998621
212.220846	1187.453346	18.524903	-0.039341	1.993023
212.182661	1179.512031	18.529907	-0.039328	1.987387
212.188711	1171.585564	18.534912	-0.039324	1.981750
212.110863	1163.681234	18.539917	-0.039304	1.976104
211.934936	1155.744661	18.544922	-0.039266	1.970408
212.061781	1147.812392	18.549927	-0.039284	1.964731
212.017309	1139.915565	18.554931	-0.039271	1.959045
212.102381	1131.968250	18.559936	-0.039281	1.953320
212.056771	1124.010979	18.564941	-0.039267	1.947556
211.999845	1116.094433	18.569946	-0.039251	1.941804
211.886681	1108.212823	18.574951	-0.039225	1.936054
211.837374	1100.282736	18.579955	-0.039211	1.930258
211.825207	1092.370022	18.584960	-0.039203	1.924462
211.887270	1084.462276	18.589965	-0.039209	1.918660
211.775631	1076.556404	18.594970	-0.039183	1.912822
211.828669	1068.637137	18.599975	-0.039188	1.906975
211.507008	1060.758313	18.604979	-0.039122	1.901098
211.390277	1052.862713	18.609984	-0.039095	1.895214
211.408629	1044.943171	18.614989	-0.039093	1.889308
211.296369	1037.027813	18.619994	-0.039067	1.883372
211.339792	1029.146137	18.624999	-0.039070	1.877461
211.216618	1021.227496	18.630003	-0.039041	1.871483
211.224422	1013.290284	18.635008	-0.039038	1.865488
211.284675	1005.382862	18.640013	-0.039043	1.859502
211.029938	997.500266	18.645018	-0.038991	1.853479
211.108306	989.585866	18.650023	-0.039000	1.847451
210.864431	981.702474	18.655027	-0.038949	1.841389
210.942780	973.797312	18.660032	-0.038958	1.835328
210.973776	965.888220	18.665037	-0.038959	1.829239
210.797992	958.000567	18.670042	-0.038921	1.823121
210.722089	950.124298	18.675047	-0.038901	1.817003
210.578900	942.216690	18.680051	-0.038869	1.810832
210.548043	934.318352	18.685056	-0.038858	1.804661
210.685544	926.421740	18.690061	-0.038878	1.798490
210.424524	918.515347	18.695066	-0.038824	1.792242
210.564378	910.579032	18.700071	-0.038845	1.785997
210.407022	902.710788	18.705075	-0.038811	1.779748
210.299554	894.829372	18.710080	-0.038785	1.773473
210.390155	886.919250	18.715085	-0.038797	1.767177
210.417583	879.019002	18.720090	-0.038796	1.760858
210.305010	871.178024	18.725095	-0.038770	1.754547
210.339351	863.271200	18.730099	-0.038771	1.748178
210.077915	855.416497	18.735104	-0.038717	1.741791
209.934047	847.567962	18.740109	-0.038685	1.735400
209.982752	839.648033	18.745114	-0.038689	1.728952
209.979853	831.786042	18.750119	-0.038683	1.722520
210.022480	823.899709	18.755123	-0.038686	1.716050
209.919102	816.017626	18.760128	-0.038661	1.709541
209.708995	808.168322	18.765133	-0.038617	1.703019
209.691786	800.285383	18.770138	-0.038608	1.696470
209.703730	792.404131	18.775143	-0.038605	1.689901
209.690898	784.524431	18.780147	-0.038597	1.683304
209.612056	776.671946	18.785152	-0.038577	1.676695
209.416427	768.825572	18.790157	-0.038535	1.670050
209.207555	760.967607	18.795162	-0.038491	1.663366
209.467195	753.070345	18.800167	-0.038534	1.656685
209.185064	745.229758	18.805171	-0.038476	1.649952
209.053370	737.380159	18.810176	-0.038447	1.643204
209.202615	729.515138	18.815181	-0.038469	1.636454
209.182000	721.576325	18.820186	-0.038460	1.629588
209.145662	713.728168	18.825191	-0.038448	1.622770
208.906351	705.906883	18.830195	-0.038398	1.615918
208.873815	698.046651	18.835200	-0.038387	1.609032
208.659084	690.234937	18.840205	-0.038341	1.602133
208.739897	682.362776	18.845210	-0.038351	1.595193
208.696644	674.518163	18.850215	-0.038338	1.588229
208.656677	666.666660	18.855219	-0.038325	1.581229
208.561667	658.841541	18.860224	-0.038302	1.574213
208.585398	650.986926	18.865229	-0.038301	1.567157
208.502189	643.158310	18.870234	-0.038280	1.560076
208.522441	635.328750	18.875239	-0.038279	1.552978
208.496279	627.458823	18.880243	-0.038268	1.545803
208.405334	619.647291	18.885248	-0.038246	1.538639
208.351862	611.814256	18.890253	-0.038231	1.531427
208.188886	603.998490	18.895258	-0.038195	1.524180
207.983683	596.222844	18.900263	-0.038152	1.516930
208.077333	588.358517	18.905267	-0.038164	1.509607
207.787117	580.575032	18.910272	-0.038105	1.502266
207.950310	572.729474	18.915277	-0.038130	1.494900
207.815393	564.913498	18.920282	-0.038099	1.487479
207.845056	557.104726	18.925287	-0.038100	1.480054
207.649129	549.298238	18.930291	-0.038058	1.472558
207.579705	541.453363	18.935296	-0.038040	1.465007
207.610355	533.654389	18.940301	-0.038040	1.457476
207.411797	525.862591	18.945306	-0.037998	1.449877
207.515893	518.060016	18.950311	-0.038012	1.442276
207.505747	510.262606	18.955315	-0.038005	1.434621
207.197071	502.505986	18.960320	-0.037942	1.426917
207.194742	494.720815	18.965325	-0.037936	1.419193
206.952983	486.951364	18.970330	-0.037886	1.411403
206.993256	479.157485	18.975335	-0.037888	1.403592
206.785803	471.410557	18.980339	-0.037844	1.395743
206.715739	463.606283	18.985344	-0.037826	1.387814
206.896732	455.798738	18.990349	-0.037854	1.379879
206.632430	448.059171	18.995354	-0.037800	1.371892
206.574100	440.296805	19.000359	-0.037784	1.363870
206.616485	432.528024	19.005363	-0.037786	1.355811
206.511526	424.772173	19.010368	-0.037762	1.347692
206.236825	417.061962	19.015373	-0.037705	1.339542
206.220212	409.293088	19.020378	-0.037697	1.331326
206.213512	401.547714	19.025383	-0.037690	1.323085
206.080768	393.811119	19.030387	-0.037660	1.314779
205.894561	385.967186	19.035392	-0.037620	1.306295
206.015236	378.229563	19.040397	-0.037638	1.297927
205.771096	370.522984	19.045402	-0.037587	1.289471
206.054662	362.765991	19.050407	-0.037635	1.281002
205.910839	355.084233	19.055411	-0.037603	1.272480
205.591153	347.412191	19.060416	-0.037538	1.263879
205.588904	339.708771	19.065421	-0.037532	1.255243
205.418960	332.023781	19.070426	-0.037495	1.246536
205.338750	324.345126	19.075431	-0.037475	1.237793
205.044213	316.677313	19.080435	-0.037415	1.228957
205.044188	308.970863	19.085440	-0.037410	1.220071
205.004349	301.295916	19.090445	-0.037397	1.211149
204.910397	293.621192	19.095450	-0.037375	1.202150
204.946523	285.956719	19.100455	-0.037376	1.193121
204.727180	278.309958	19.105459	-0.037330	1.183992
204.584983	270.680367	19.110464	-0.037299	1.174829
204.650697	263.013112	19.115469	-0.037306	1.165592
204.536938	255.390898	19.120474	-0.037279	1.156297
204.568358	247.712549	19.125479	-0.037280	1.146890
204.159106	240.143635	19.130483	-0.037199	1.137446
204.095695	232.522948	19.135488	-0.037182	1.127932
204.173287	224.901551	19.140493	-0.037191	1.118368
203.575635	217.383347	19.145498	-0.037074	1.108704
203.383588	209.811924	19.150503	-0.037034	1.098976
203.042274	202.263664	19.155507	-0.036965	1.089158
202.887004	194.697833	19.160512	-0.036931	1.079270
202.425086	187.190682	19.165517	-0.036840	1.069298
201.963311	179.676476	19.170522	-0.036749	1.059222
201.676847	172.153378	19.175527	-0.036690	1.049078
201.252519	164.662496	19.180531	-0.036606	1.038846
200.713643	157.193132	19.185536	-0.036501	1.028514
200.487701	149.687546	19.190541	-0.036454	1.018103
200.000585	142.223905	19.195546	-0.036358	1.007578
199.496934	134.799000	19.200551	-0.036259	0.996994
199.084900	127.306234	19.205555	-0.036177	0.986221
198.691250	119.864032	19.210560	-0.036099	0.975406
198.093592	112.471316	19.215565	-0.035983	0.964491
197.632612	105.074231	19.220570	-0.035892	0.953479
197.388003	97.647268	19.225575	-0.035841	0.942350
196.621812	90.329021	19.230579	-0.035694	0.931115
196.184476	82.969303	19.235584	-0.035607	0.919766
195.986510	75.580886	19.240589	-0.035565	0.908296
195.373636	68.283782	19.245594	-0.035446	0.896709
194.818642	61.224145	19.250599	-0.035338	0.885364