Fri Mar 12 12:54:22 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.775961	-0.100219	0.000000	0.000013	0.718012

0.715497	-0.085410	0.005005	0.000024	0.718020
0.846987	-0.113164	0.010010	-0.000000	0.718011
1.049024	-0.145386	0.015014	-0.000038	0.718018
0.893182	-0.120304	0.020019	-0.000008	0.718012
0.721185	-0.089263	0.025024	0.000024	0.718013
1.028082	-0.141466	0.030029	-0.000033	0.718017
0.815111	-0.107788	0.035034	0.000007	0.718008
0.818188	-0.104178	0.040038	0.000006	0.718016
0.976381	-0.134990	0.045043	-0.000023	0.718011
0.931308	-0.128215	0.050048	-0.000014	0.718008
0.864722	-0.111999	0.055053	-0.000002	0.718016
0.936681	-0.129229	0.060058	-0.000015	0.718007
1.020463	-0.138848	0.065062	-0.000030	0.718017
0.832316	-0.106629	0.070067	0.000005	0.718014
0.931105	-0.211418	0.075072	-0.000013	0.717842
1.058481	-0.304696	0.080077	-0.000037	0.717702
0.895217	-0.279079	0.085082	-0.000006	0.717695
0.628793	-0.227191	0.090086	0.000043	0.717703
0.829817	-0.264447	0.095091	0.000006	0.717700
0.716533	-0.244811	0.100096	0.000027	0.717699
0.695317	-0.237152	0.105101	0.000032	0.717706
0.873948	-0.422314	0.110106	-0.000001	0.717402
0.918344	-0.441617	0.115110	-0.000009	0.717379
0.776658	-0.417158	0.120115	0.000017	0.717378
0.708257	-0.406226	0.125120	0.000030	0.717375
0.908876	-0.439226	0.130125	-0.000007	0.717380
0.791792	-0.555670	0.135130	0.000015	0.717108
0.579309	-0.528816	0.140134	0.000055	0.717086
0.654946	-0.545749	0.145139	0.000041	0.717079
0.839946	-0.579283	0.150144	0.000006	0.717077
0.657161	-0.630687	0.155149	0.000041	0.716911
0.490938	-0.685100	0.160154	0.000072	0.716744
0.809656	-0.738471	0.165158	0.000013	0.716750
0.730264	-0.725737	0.170163	0.000028	0.716747
0.671052	-0.824224	0.175168	0.000039	0.716531
1.001508	-0.924188	0.180173	-0.000022	0.716449
0.807708	-0.894226	0.185178	0.000014	0.716440
0.778340	-0.942659	0.190182	0.000020	0.716333
0.917738	-1.069647	0.195187	-0.000006	0.716131
0.906153	-1.069384	0.200192	-0.000004	0.716127
0.674651	-1.062485	0.205197	0.000039	0.716058
0.574353	-1.133699	0.210202	0.000058	0.715882
0.932929	-1.195792	0.215206	-0.000008	0.715885
1.072254	-1.294355	0.220211	-0.000034	0.715738
0.720410	-1.330480	0.225216	0.000032	0.715542
0.579773	-1.301715	0.230221	0.000058	0.715549
0.460848	-1.396463	0.235226	0.000081	0.715319
0.373949	-1.425198	0.240230	0.000097	0.715231
0.249202	-1.403239	0.245235	0.000120	0.715230
0.310143	-1.571431	0.250240	0.000109	0.714917
0.302725	-1.573637	0.255245	0.000111	0.714910
0.083133	-1.587004	0.260250	0.000152	0.714806
0.482534	-1.757028	0.265254	0.000078	0.714609
0.629165	-1.786403	0.270259	0.000051	0.714602
0.286403	-1.878842	0.275264	0.000115	0.714297
-0.034119	-1.831942	0.280269	0.000175	0.714276
-0.132037	-1.888348	0.285274	0.000193	0.714129
0.027443	-1.996527	0.290278	0.000164	0.713971
-0.096981	-1.990176	0.295283	0.000187	0.713939
-0.078042	-2.140550	0.300288	0.000184	0.713646
-0.214306	-2.113238	0.305293	0.000209	0.713652
-0.925578	-2.105156	0.310298	0.000342	0.713416
-1.256725	-2.073065	0.315302	0.000404	0.713362
-1.378330	-2.082346	0.320307	0.000426	0.713300
-2.063173	-2.099854	0.325312	0.000554	0.713022
-1.985693	-2.111176	0.330317	0.000540	0.713027
-2.801195	-2.012572	0.335322	0.000692	0.712933
-3.274817	-2.040507	0.340326	0.000780	0.712709
-2.754103	-2.134412	0.345331	0.000684	0.712707
-3.598342	-1.984014	0.350336	0.000841	0.712706
-3.629420	-2.135986	0.355341	0.000847	0.712392
-3.991864	-2.076643	0.360346	0.000915	0.712382
-4.365470	-2.006809	0.365350	0.000984	0.712388
-4.132388	-2.109882	0.370355	0.000941	0.712265
-5.198684	-2.010948	0.375360	0.001140	0.712083
-4.723388	-2.091710	0.380365	0.001051	0.712091
-5.250419	-2.002645	0.385370	0.001150	0.712081
-5.127835	-2.082477	0.390374	0.001127	0.711965
-5.916311	-2.044200	0.395379	0.001274	0.711761
-6.142369	-2.006608	0.400384	0.001316	0.711755
-5.915884	-2.042881	0.405389	0.001274	0.711763
-5.858143	-2.057347	0.410394	0.001264	0.711754
-6.074519	-2.146731	0.415398	0.001304	0.711499
-7.189072	-1.971043	0.420403	0.001512	0.711453
-7.035542	-2.000111	0.425408	0.001483	0.711449
-6.248164	-2.136335	0.430413	0.001337	0.711457
-7.067491	-1.995567	0.435418	0.001490	0.711446
-7.334056	-2.091476	0.440422	0.001540	0.711159
-7.364428	-2.097120	0.445427	0.001546	0.711137
-8.010085	-1.985612	0.450432	0.001666	0.711130
-7.440909	-2.080846	0.455437	0.001560	0.711142
-7.672781	-2.044013	0.460442	0.001603	0.711132
-8.034820	-2.076040	0.465446	0.001671	0.710939
-8.659979	-1.998601	0.470451	0.001788	0.710871
-8.783038	-1.978653	0.475456	0.001811	0.710867
-8.229606	-2.073353	0.480461	0.001708	0.710874
-8.903218	-1.956039	0.485466	0.001833	0.710869
-8.552386	-2.015574	0.490470	0.001768	0.710874
-8.721598	-2.141254	0.495475	0.001800	0.710563
-9.833647	-1.958973	0.500480	0.002007	0.710531
-9.536126	-2.009089	0.505485	0.001952	0.710536
-9.040845	-2.101715	0.510490	0.001860	0.710527
-9.382248	-2.038557	0.515494	0.001924	0.710531
-9.463740	-2.024530	0.520499	0.001939	0.710530
-10.044787	-2.078222	0.525504	0.002047	0.710216
-10.022579	-2.077519	0.530509	0.002043	0.710225
-10.512713	-1.995003	0.535514	0.002135	0.710215
-10.234001	-2.043370	0.540518	0.002083	0.710217
-10.382077	-2.015875	0.545523	0.002111	0.710219
-10.619958	-1.976204	0.550528	0.002155	0.710213
-10.385778	-2.116926	0.555533	0.002112	0.710015
-11.709952	-1.943829	0.560538	0.002359	0.709889
-11.208552	-2.030557	0.565542	0.002265	0.709894
-11.223797	-2.027827	0.570547	0.002268	0.709893
-11.606660	-1.960910	0.575552	0.002340	0.709890
-11.158793	-2.039074	0.580557	0.002257	0.709893
-11.440089	-1.991663	0.585562	0.002309	0.709888
-11.771852	-2.045334	0.590566	0.002371	0.709662
-12.080894	-2.023455	0.595571	0.002429	0.709595
-12.312892	-1.983267	0.600576	0.002472	0.709592
-12.363028	-1.970105	0.605581	0.002482	0.709600
-12.218462	-2.000578	0.610586	0.002455	0.709591
-12.001830	-2.036090	0.615590	0.002415	0.709596
-12.407895	-1.963553	0.620595	0.002491	0.709596
-12.859755	-2.019760	0.625600	0.002575	0.709323
-12.918775	-2.035714	0.630605	0.002586	0.709269
-13.225467	-1.985411	0.635610	0.002643	0.709260
-13.321485	-1.966062	0.640614	0.002662	0.709264
-13.075826	-2.009792	0.645619	0.002616	0.709264
-13.231805	-1.985764	0.650624	0.002645	0.709256
-13.185128	-1.988570	0.655629	0.002637	0.709267
-13.376547	-2.053539	0.660634	0.002673	0.709068
-14.106459	-1.980051	0.665638	0.002809	0.708955
-13.910023	-2.014424	0.670643	0.002772	0.708956
-14.168907	-1.969558	0.675648	0.002821	0.708953
-13.884718	-2.016686	0.680653	0.002768	0.708959
-14.154206	-1.974647	0.685658	0.002818	0.708947
-14.116658	-1.976843	0.690662	0.002811	0.708956
-13.994865	-2.094275	0.695667	0.002789	0.708764
-15.151435	-1.954030	0.700672	0.003004	0.708631
-15.097758	-1.959180	0.705677	0.002995	0.708640
-14.992964	-1.982209	0.710682	0.002975	0.708631
-14.945839	-1.989621	0.715686	0.002967	0.708633
-14.829824	-2.009350	0.720691	0.002945	0.708634
-15.301583	-1.927048	0.725696	0.003033	0.708630
-14.969473	-2.037115	0.730701	0.002972	0.708528
-15.851152	-1.972987	0.735706	0.003136	0.708341
-16.130905	-1.921010	0.740710	0.003188	0.708345
-16.037837	-1.936883	0.745715	0.003171	0.708346
-15.825831	-1.977617	0.750720	0.003132	0.708340
-15.907338	-1.958324	0.755725	0.003147	0.708349
-16.106591	-1.926576	0.760730	0.003184	0.708341
-15.757055	-1.990147	0.765734	0.003119	0.708338
-16.330101	-2.051319	0.770739	0.003226	0.708011
-17.172571	-1.905858	0.775744	0.003383	0.708001
-16.939045	-1.941005	0.780749	0.003340	0.708014
-16.771912	-1.975530	0.785754	0.003309	0.708004
-17.068036	-1.920635	0.790758	0.003364	0.708008
-16.577224	-2.007207	0.795763	0.003273	0.708009
-16.693248	-1.988538	0.800768	0.003295	0.708005
-17.315705	-1.987739	0.805773	0.003411	0.707784
-18.167501	-1.882561	0.810778	0.003570	0.707690
-17.591472	-1.983158	0.815782	0.003463	0.707694
-17.569126	-1.985415	0.820787	0.003459	0.707697
-18.444209	-1.833512	0.825792	0.003622	0.707688
-17.696324	-1.961666	0.830797	0.003483	0.707698
-17.366280	-2.022114	0.835802	0.003422	0.707695
-17.941460	-1.960321	0.840806	0.003529	0.707613
-18.797977	-1.925785	0.845811	0.003688	0.707375
-18.563205	-1.970886	0.850816	0.003645	0.707368
-18.834684	-1.917504	0.855821	0.003696	0.707378
-18.780825	-1.931641	0.860826	0.003686	0.707369
-18.570711	-1.967719	0.865830	0.003647	0.707371
-18.385202	-1.997971	0.870835	0.003613	0.707376
-18.874104	-1.914469	0.875840	0.003704	0.707369
-19.109730	-2.000708	0.880845	0.003748	0.707111
-19.441857	-1.959106	0.885850	0.003810	0.707075
-19.507709	-1.943933	0.890854	0.003822	0.707082
-19.271705	-1.983654	0.895859	0.003778	0.707086
-19.498841	-1.948519	0.900864	0.003821	0.707075
-19.242227	-1.989893	0.905869	0.003773	0.707084
-19.416250	-1.981720	0.910874	0.003806	0.707037
-19.981295	-2.022777	0.915878	0.003911	0.706752
-20.241184	-1.975116	0.920883	0.003960	0.706755
-21.083962	-1.828645	0.925888	0.004117	0.706747
-20.467342	-1.933649	0.930893	0.004002	0.706756
-20.320035	-1.964323	0.935898	0.003975	0.706747
-20.812663	-1.874632	0.940902	0.004067	0.706751
-20.707718	-1.890450	0.945907	0.004048	0.706756
-20.640333	-1.994922	0.950912	0.004035	0.706570
-21.370011	-1.925593	0.955917	0.004171	0.706448
-21.446726	-1.915867	0.960922	0.004186	0.706439
-21.449724	-1.913299	0.965926	0.004186	0.706443
-21.285758	-1.940144	0.970931	0.004156	0.706447
-21.512005	-1.905393	0.975936	0.004198	0.706436
-21.338342	-1.930549	0.980941	0.004166	0.706447
-21.391536	-1.981370	0.985946	0.004176	0.706326
-22.309053	-1.918562	0.990950	0.004347	0.706123
-21.826512	-2.002353	0.995955	0.004258	0.706127
-22.303186	-1.919037	1.000960	0.004347	0.706123
-22.343484	-1.908928	1.005965	0.004354	0.706129
-22.305754	-1.919212	1.010970	0.004347	0.706121
-22.498301	-1.883321	1.015974	0.004383	0.706124
-21.964562	-2.018788	1.020979	0.004284	0.706043
-23.074796	-1.915216	1.025984	0.004491	0.705853
-22.901687	-1.939153	1.030989	0.004459	0.705866
-22.783895	-1.963242	1.035994	0.004437	0.705860
-22.891201	-1.944139	1.040998	0.004457	0.705859
-22.999389	-1.921540	1.046003	0.004478	0.705866
-23.113385	-1.906134	1.051008	0.004499	0.705855
-23.026334	-2.033037	1.056013	0.004483	0.705631
-24.003568	-1.914636	1.061018	0.004665	0.705518
-24.110656	-1.893864	1.066022	0.004685	0.705521
-23.523565	-1.997385	1.071027	0.004576	0.705523
-24.021167	-1.912427	1.076032	0.004669	0.705516
-23.907392	-1.926645	1.081037	0.004648	0.705527
-23.709690	-1.966374	1.086042	0.004611	0.705518
-24.266369	-2.003397	1.091046	0.004715	0.705243
-24.763020	-1.930198	1.096051	0.004808	0.705212
-24.685537	-1.947138	1.101056	0.004794	0.705206
-24.270595	-2.017685	1.106061	0.004717	0.705212
-24.734271	-1.939275	1.111066	0.004803	0.705203
-24.792281	-1.928222	1.116070	0.004814	0.705204
-24.324794	-2.054581	1.121075	0.004727	0.705117
-25.649014	-1.936396	1.126080	0.004974	0.704880
-25.504594	-1.958060	1.131085	0.004947	0.704888
-25.453641	-1.967285	1.136090	0.004938	0.704887
-25.471882	-1.964794	1.141094	0.004942	0.704885
-25.602488	-1.940837	1.146099	0.004966	0.704886
-25.871403	-1.895711	1.151104	0.005016	0.704880
-25.468834	-2.025123	1.156109	0.004942	0.704764
-26.449584	-1.938861	1.161114	0.005124	0.704585
-26.520120	-1.926156	1.166118	0.005138	0.704585
-26.353093	-1.952898	1.171123	0.005107	0.704590
-26.754189	-1.885289	1.176128	0.005182	0.704582
-26.537275	-1.918988	1.181133	0.005141	0.704592
-26.641176	-1.903201	1.186138	0.005161	0.704586
-26.512656	-1.964755	1.191142	0.005137	0.704508
-27.334529	-1.940387	1.196147	0.005290	0.704261
-27.183155	-1.971774	1.201152	0.005262	0.704252
-27.411077	-1.926712	1.206157	0.005305	0.704261
-27.686741	-1.880726	1.211162	0.005356	0.704254
-27.585673	-1.898382	1.216166	0.005338	0.704254
-27.057504	-1.989164	1.221171	0.005240	0.704261
-27.346571	-1.962275	1.226176	0.005294	0.704211
-28.119618	-1.952592	1.231181	0.005438	0.703952
-28.180108	-1.942258	1.236186	0.005449	0.703951
-28.156157	-1.948333	1.241190	0.005445	0.703947
-28.244057	-1.927965	1.246195	0.005461	0.703956
-28.452797	-1.894295	1.251200	0.005500	0.703949
-28.164471	-1.942745	1.256205	0.005447	0.703954
-28.212084	-1.958853	1.261210	0.005456	0.703904
-29.283123	-1.902633	1.266214	0.005656	0.703632
-29.061723	-1.940932	1.271219	0.005615	0.703634
-29.473996	-1.871435	1.276224	0.005691	0.703626
-29.182529	-1.919906	1.281229	0.005637	0.703632
-28.947101	-1.963336	1.286234	0.005594	0.703629
-29.181360	-1.921014	1.291238	0.005638	0.703630
-29.016884	-1.948390	1.296243	0.005607	0.703633
-29.577782	-1.993391	1.301248	0.005712	0.703340
-29.443080	-2.016542	1.306253	0.005687	0.703342
-29.919362	-1.933929	1.311258	0.005776	0.703337
-30.201040	-1.883809	1.316262	0.005828	0.703336
-29.655466	-1.977163	1.321267	0.005727	0.703344
-29.858092	-1.944424	1.326272	0.005765	0.703337
-29.933229	-2.009605	1.331277	0.005779	0.703178
-30.849779	-1.931045	1.336282	0.005950	0.703006
-30.620506	-1.974112	1.341286	0.005907	0.703001
-30.617813	-1.971332	1.346291	0.005907	0.703007
-31.194656	-1.872100	1.351296	0.006014	0.703000
-30.509603	-1.989592	1.356301	0.005887	0.703009
-30.388824	-2.013740	1.361306	0.005865	0.703003
-31.366360	-1.970949	1.366310	0.006047	0.702737
-31.552082	-1.958910	1.371315	0.006082	0.702694
-31.705641	-1.935725	1.376320	0.006111	0.702686
-31.462168	-1.974488	1.381325	0.006065	0.702695
-31.603469	-1.951481	1.386330	0.006092	0.702690
-31.513979	-1.967693	1.391334	0.006075	0.702689
-31.482096	-1.980354	1.396339	0.006070	0.702675
-32.452485	-1.962280	1.401344	0.006251	0.702361
-32.169080	-2.007201	1.406349	0.006198	0.702372
-32.365052	-1.974637	1.411354	0.006235	0.702367
-32.685084	-1.918948	1.416358	0.006294	0.702364
-32.176321	-2.006059	1.421363	0.006200	0.702371
-32.286703	-1.989953	1.426368	0.006221	0.702363
-32.493547	-2.012467	1.431373	0.006259	0.702243
-33.471532	-1.923827	1.436378	0.006441	0.702069
-32.908968	-2.024741	1.441382	0.006337	0.702067
-32.887857	-2.025674	1.446387	0.006333	0.702073
-33.521618	-1.916782	1.451392	0.006451	0.702064
-33.072210	-1.992463	1.456397	0.006368	0.702073
-33.014299	-2.007020	1.461402	0.006357	0.702064
-33.864958	-1.994795	1.466406	0.006516	0.701781
-34.020626	-1.985653	1.471411	0.006545	0.701743
-34.167784	-1.964065	1.476416	0.006573	0.701734
-33.904795	-2.005815	1.481421	0.006524	0.701744
-34.357484	-1.926507	1.486426	0.006608	0.701740
-34.300856	-1.937554	1.491430	0.006598	0.701738
-34.126958	-1.966041	1.496435	0.006566	0.701743
-34.933173	-1.957930	1.501440	0.006716	0.701468
-34.919956	-1.975309	1.506445	0.006714	0.701437
-34.985314	-1.964642	1.511450	0.006726	0.701435
-35.150091	-1.936555	1.516454	0.006757	0.701432
-35.172613	-1.930250	1.521459	0.006761	0.701436
-35.104257	-1.945123	1.526464	0.006749	0.701431
-34.933582	-1.971764	1.531469	0.006717	0.701438
-35.441901	-1.994936	1.536474	0.006812	0.701207
-36.111344	-1.919555	1.541478	0.006937	0.701118
-35.393996	-2.045031	1.546483	0.006803	0.701122
-35.829192	-1.971882	1.551488	0.006885	0.701113
-36.025285	-1.931620	1.556493	0.006921	0.701123
-35.659585	-1.998744	1.561498	0.006853	0.701119
-35.787471	-1.990375	1.566502	0.006877	0.701089
-36.506963	-1.968239	1.571507	0.007011	0.700874
-36.454331	-1.981847	1.576512	0.007002	0.700865
-36.410754	-1.986829	1.581517	0.006994	0.700870
-36.635613	-1.948488	1.586522	0.007036	0.700867
-36.482858	-1.974866	1.591526	0.007008	0.700868
-36.443596	-1.978347	1.596531	0.007001	0.700875
-36.968200	-2.004446	1.601536	0.007098	0.700632
-37.662673	-1.929910	1.606541	0.007228	0.700532
-37.103299	-2.029610	1.611546	0.007124	0.700531
-37.373919	-1.984069	1.616550	0.007174	0.700526
-37.562286	-1.946843	1.621555	0.007210	0.700533
-37.320953	-1.992560	1.626560	0.007165	0.700527
-37.204588	-2.041324	1.631565	0.007144	0.700470
-38.419844	-1.949955	1.636570	0.007370	0.700215
-38.466928	-1.941313	1.641574	0.007379	0.700215
-38.206933	-1.985778	1.646579	0.007331	0.700219
-38.743728	-1.893575	1.651584	0.007431	0.700211
-38.576242	-1.920234	1.656589	0.007400	0.700217
-38.327083	-1.965653	1.661594	0.007354	0.700215
-38.343960	-1.966592	1.666598	0.007357	0.700207
-38.908500	-2.019795	1.671603	0.007462	0.699894
-39.287080	-1.954496	1.676608	0.007533	0.699889
-39.283026	-1.953204	1.681613	0.007532	0.699893
-39.158533	-1.975737	1.686618	0.007509	0.699892
-39.459681	-1.922631	1.691622	0.007565	0.699891
-39.263292	-1.954754	1.696627	0.007529	0.699896
-39.449901	-1.925999	1.701632	0.007564	0.699887
-39.799148	-2.005948	1.706637	0.007629	0.699598
-39.929202	-1.984239	1.711642	0.007654	0.699594
-40.283631	-1.923398	1.716646	0.007720	0.699589
-40.029410	-1.964876	1.721651	0.007673	0.699597
-40.215848	-1.934302	1.726656	0.007708	0.699591
-39.914658	-1.985733	1.731661	0.007652	0.699595
-40.157547	-1.981116	1.736666	0.007697	0.699516
-41.258073	-1.910898	1.741670	0.007902	0.699260
-40.447711	-2.052332	1.746675	0.007751	0.699266
-41.068793	-1.944701	1.751680	0.007867	0.699259
-41.184863	-1.921334	1.756685	0.007889	0.699264
-40.699399	-2.008629	1.761690	0.007799	0.699262
-41.195157	-1.921158	1.766694	0.007891	0.699260
-41.057513	-1.992224	1.771699	0.007866	0.699165
-41.945175	-1.939428	1.776704	0.008031	0.698951
-41.638804	-1.990827	1.781709	0.007974	0.698957
-41.860762	-1.952224	1.786714	0.008016	0.698954
-42.303251	-1.876210	1.791718	0.008098	0.698948
-41.483963	-2.017475	1.796723	0.007946	0.698958
-41.905293	-1.946233	1.801728	0.008025	0.698949
-41.981396	-1.987107	1.806733	0.008039	0.698839
-42.603910	-1.975747	1.811738	0.008155	0.698636
-42.363888	-2.019001	1.816742	0.008111	0.698634
-42.749669	-1.947455	1.821747	0.008183	0.698640
-42.665709	-1.966752	1.826752	0.008167	0.698630
-42.395894	-2.011941	1.831757	0.008117	0.698636
-42.496211	-1.992728	1.836762	0.008136	0.698638
-43.124070	-1.994124	1.841766	0.008253	0.698408
-43.351988	-1.982088	1.846771	0.008296	0.698349
-43.614699	-1.939361	1.851776	0.008345	0.698340
-43.465035	-1.962163	1.856781	0.008317	0.698348
-43.381431	-1.977289	1.861786	0.008302	0.698347
-43.436861	-1.968232	1.866790	0.008312	0.698345
-43.328081	-2.007419	1.871795	0.008292	0.698304
-44.381881	-1.963626	1.876800	0.008489	0.698011
-44.045821	-2.020558	1.881805	0.008426	0.698017
-44.297648	-1.977429	1.886810	0.008473	0.698013
-44.754762	-1.897800	1.891814	0.008558	0.698008
-44.295190	-1.975151	1.896819	0.008473	0.698017
-44.411306	-1.959258	1.901824	0.008495	0.698007
-44.331926	-2.015667	1.906829	0.008480	0.697921
-45.218695	-1.967267	1.911834	0.008646	0.697697
-44.999222	-2.009886	1.916838	0.008605	0.697690
-45.425223	-1.927255	1.921843	0.008684	0.697703
-45.577318	-1.905094	1.926848	0.008713	0.697692
-45.121012	-1.983362	1.931853	0.008628	0.697699
-45.024091	-1.998947	1.936858	0.008610	0.697702
-45.476491	-1.965507	1.941862	0.008695	0.697605
-45.898191	-2.000081	1.946867	0.008773	0.697381
-45.608596	-2.056356	1.951872	0.008720	0.697371
-46.260809	-1.937554	1.956877	0.008841	0.697376
-46.258825	-1.937892	1.961882	0.008841	0.697376
-46.066948	-1.974247	1.966886	0.008805	0.697371
-46.054222	-1.970983	1.971891	0.008803	0.697382
-46.426204	-1.972016	1.976896	0.008873	0.697244
-47.052231	-1.939365	1.981901	0.008989	0.697083
-46.571800	-2.023895	1.986906	0.008900	0.697085
-47.221308	-1.912545	1.991910	0.009021	0.697076
-46.876912	-1.969095	1.996915	0.008957	0.697085
-46.857262	-1.975547	2.001920	0.008954	0.697079

-47.193713	-2.011637	2.011917	0.009017	0.696882
-47.793536	-1.969441	2.021914	0.009129	0.696750
-47.585265	-2.006637	2.031910	0.009091	0.696749
-48.072992	-1.917806	2.041907	0.009182	0.696752
-47.736955	-1.978367	2.051904	0.009119	0.696750
-47.929162	-1.943476	2.061901	0.009156	0.696750
-47.794485	-1.967276	2.071898	0.009131	0.696750
-47.649750	-1.992526	2.081894	0.009104	0.696751
-47.823621	-1.906928	2.091891	0.009137	0.696861
-46.878841	-1.969395	2.101888	0.008961	0.697077
-46.991265	-1.949119	2.111885	0.008983	0.697076
-46.852573	-1.971449	2.121882	0.008957	0.697081
-46.710789	-1.994906	2.131878	0.008931	0.697084
-46.938807	-1.954893	2.141875	0.008974	0.697082
-46.581831	-2.019035	2.151872	0.008908	0.697080
-46.998974	-1.928758	2.161869	0.008986	0.697112
-45.830170	-2.007084	2.171866	0.008769	0.697376
-45.843911	-2.003260	2.181862	0.008772	0.697378
-46.037303	-1.970767	2.191859	0.008808	0.697373
-45.984139	-1.978455	2.201856	0.008798	0.697376
-45.891439	-1.938704	2.211853	0.008781	0.697490
-45.133761	-1.970110	2.221850	0.008641	0.697701
-45.063161	-1.981175	2.231846	0.008628	0.697703
-45.323688	-1.933370	2.241843	0.008677	0.697705
-44.788664	-1.946761	2.251840	0.008577	0.697872
-44.517447	-1.924638	2.261837	0.008527	0.698014
-44.273634	-1.968440	2.271834	0.008482	0.698013
-44.445284	-1.938716	2.281830	0.008515	0.698011
-43.526308	-1.962113	2.291827	0.008344	0.698296
-43.456610	-1.947695	2.301824	0.008331	0.698350
-43.442696	-1.949493	2.311821	0.008329	0.698350
-43.344708	-1.949878	2.321818	0.008311	0.698384
-42.823860	-1.914948	2.331814	0.008214	0.698644
-42.547752	-1.965701	2.341811	0.008163	0.698640
-42.530215	-1.970297	2.351808	0.008161	0.698636
-42.375216	-1.907562	2.361805	0.008132	0.698819
-41.500004	-1.997635	2.371802	0.007969	0.698953
-41.989253	-1.908809	2.381798	0.008061	0.698955
-41.625039	-1.961160	2.391795	0.007993	0.698980
-41.065310	-1.922235	2.401792	0.007889	0.699261
-40.944411	-1.942574	2.411789	0.007867	0.699263
-40.880131	-1.952161	2.421786	0.007856	0.699266
-40.441998	-1.915547	2.431782	0.007774	0.699499
-40.125843	-1.924169	2.441779	0.007716	0.699595
-40.040131	-1.939810	2.451776	0.007700	0.699594
-39.900438	-1.935165	2.461773	0.007675	0.699653
-39.012973	-1.975458	2.471770	0.007510	0.699892
-39.246490	-1.932743	2.481766	0.007554	0.699893
-39.110368	-1.957221	2.491763	0.007529	0.699892
-38.735656	-1.906142	2.501760	0.007459	0.700131
-38.336493	-1.936224	2.511757	0.007385	0.700213
-38.149635	-1.967399	2.521754	0.007351	0.700217
-38.147535	-1.934797	2.531750	0.007351	0.700283
-37.415737	-1.941275	2.541747	0.007215	0.700534
-37.551814	-1.917557	2.551744	0.007241	0.700532
-37.530827	-1.922466	2.561741	0.007237	0.700529
-36.644246	-1.936945	2.571738	0.007072	0.700819
-36.662859	-1.906985	2.581734	0.007076	0.700873
-36.410794	-1.951674	2.591731	0.007030	0.700873
-36.514970	-1.900744	2.601728	0.007049	0.700937
-35.822364	-1.934912	2.611725	0.006921	0.701118
-35.763840	-1.943081	2.621722	0.006910	0.701122
-35.869193	-1.923378	2.631718	0.006930	0.701123
-35.086153	-1.908491	2.641715	0.006785	0.701435
-35.165385	-1.894681	2.651712	0.006800	0.701434
-34.939821	-1.933562	2.661709	0.006758	0.701436
-34.484360	-1.901277	2.671706	0.006674	0.701665
-34.126549	-1.924927	2.681702	0.006607	0.701745
-33.992361	-1.949405	2.691699	0.006583	0.701744
-34.054107	-1.885607	2.701696	0.006595	0.701850
-33.128943	-1.941949	2.711693	0.006423	0.702069
-33.220741	-1.923813	2.721690	0.006440	0.702072
-33.147555	-1.936410	2.731686	0.006427	0.702072
-32.447695	-1.928536	2.741683	0.006297	0.702339
-32.571599	-1.893272	2.751680	0.006320	0.702365
-32.345159	-1.933310	2.761677	0.006278	0.702365
-32.000633	-1.911398	2.771674	0.006215	0.702533
-31.075630	-1.998380	2.781670	0.006043	0.702690
-31.217100	-1.974249	2.791667	0.006070	0.702687
-31.631072	-1.899789	2.801664	0.006147	0.702688
-30.742304	-1.924698	2.811661	0.005982	0.702957
-30.658869	-1.917105	2.821658	0.005967	0.703002
-30.607938	-1.924687	2.831654	0.005957	0.703004
-30.145883	-1.932976	2.841651	0.005872	0.703153
-29.478656	-1.960486	2.851648	0.005748	0.703337
-29.375875	-1.979287	2.861645	0.005729	0.703335
-29.703365	-1.918624	2.871642	0.005790	0.703339
-28.815488	-1.990520	2.881638	0.005626	0.703513
-28.692018	-1.952442	2.891635	0.005603	0.703633
-28.896759	-1.917034	2.901632	0.005641	0.703631
-28.557808	-1.970893	2.911629	0.005579	0.703643
-27.864229	-1.942046	2.921626	0.005450	0.703950
-27.611139	-1.986212	2.931622	0.005403	0.703951
-27.828212	-1.946282	2.941619	0.005444	0.703953
-27.721043	-1.907970	2.951616	0.005424	0.704068
-26.879060	-1.964528	2.961613	0.005268	0.704256
-27.074742	-1.927986	2.971610	0.005305	0.704259
-26.629821	-2.005962	2.981606	0.005222	0.704261
-26.381873	-1.900005	2.991603	0.005176	0.704563
-26.026506	-1.951426	3.001600	0.005110	0.704586
-25.984380	-1.956970	3.011597	0.005103	0.704590
-25.909918	-1.900243	3.021594	0.005089	0.704730
-25.105049	-1.964443	3.031590	0.004940	0.704889
-25.317918	-1.927242	3.041587	0.004980	0.704887
-25.091510	-1.966453	3.051584	0.004938	0.704888
-24.446941	-1.922793	3.061581	0.004818	0.705207
-24.377466	-1.934724	3.071578	0.004806	0.705207
-24.270569	-1.953560	3.081574	0.004786	0.705207
-24.143096	-1.881717	3.091571	0.004763	0.705397
-23.414359	-1.949583	3.101568	0.004628	0.705521
-23.610167	-1.915621	3.111565	0.004664	0.705518
-23.358028	-1.933393	3.121562	0.004618	0.705572
-22.693680	-1.907549	3.131558	0.004494	0.705862
-22.593398	-1.926215	3.141555	0.004476	0.705860
-22.522513	-1.939058	3.151552	0.004463	0.705858
-22.098352	-1.923082	3.161549	0.004385	0.706042
-21.873236	-1.921010	3.171546	0.004343	0.706126
-21.906221	-1.915454	3.181542	0.004350	0.706125
-21.800679	-1.882653	3.191539	0.004330	0.706228
-20.780494	-1.960543	3.201536	0.004141	0.706436
-20.843032	-1.947580	3.211533	0.004153	0.706439
-20.850388	-1.943248	3.221530	0.004154	0.706444
-20.295713	-1.916180	3.231526	0.004051	0.706697
-20.046741	-1.934193	3.241523	0.004005	0.706749
-20.100174	-1.925888	3.251520	0.004016	0.706746
-19.997566	-1.875510	3.261517	0.003997	0.706883
-19.071195	-1.943148	3.271514	0.003825	0.707078
-19.219211	-1.915882	3.281510	0.003853	0.707079
-19.252168	-1.907178	3.291507	0.003859	0.707084
-18.530862	-1.891424	3.301504	0.003725	0.707373
-18.376138	-1.918665	3.311501	0.003697	0.707373
-18.258720	-1.938089	3.321498	0.003675	0.707376
-17.850428	-1.912332	3.331494	0.003600	0.707573
-17.429767	-1.925222	3.341491	0.003522	0.707697
-17.256285	-1.956858	3.351488	0.003490	0.707695
-17.629277	-1.878505	3.361485	0.003560	0.707718
-16.516904	-1.929857	3.371482	0.003353	0.708012
-16.470924	-1.937520	3.381478	0.003345	0.708012
-16.499772	-1.932626	3.391475	0.003350	0.708011
-16.182236	-1.906662	3.401472	0.003291	0.708176
-15.667370	-1.911988	3.411469	0.003196	0.708348
-15.516855	-1.936956	3.421466	0.003168	0.708351
-15.664908	-1.911128	3.431462	0.003196	0.708349
-14.884521	-1.918849	3.441459	0.003051	0.708612
-14.791088	-1.922835	3.451456	0.003034	0.708637
-14.875899	-1.907304	3.461453	0.003050	0.708637
-14.450575	-1.914561	3.471450	0.002972	0.708773
-13.908468	-1.919509	3.481446	0.002871	0.708956
-13.784243	-1.941897	3.491443	0.002848	0.708955
-13.948541	-1.913956	3.501440	0.002879	0.708952
-13.237421	-1.899720	3.511437	0.002747	0.709233
-12.928855	-1.939653	3.521434	0.002690	0.709263
-13.235690	-1.883850	3.531430	0.002747	0.709264
-12.592922	-1.914052	3.541427	0.002628	0.709432
-12.087662	-1.922577	3.551424	0.002534	0.709595
-11.941614	-1.948971	3.561421	0.002508	0.709593
-11.666194	-1.996937	3.571418	0.002457	0.709595
-11.717510	-1.889678	3.581414	0.002466	0.709790
-10.818305	-1.997801	3.591411	0.002299	0.709894
-11.131461	-1.942437	3.601408	0.002358	0.709892
-10.905872	-1.982733	3.611405	0.002316	0.709892
-10.483768	-1.904781	3.621402	0.002238	0.710197
-10.256377	-1.933312	3.631398	0.002196	0.710220
-10.067961	-1.967413	3.641395	0.002162	0.710219
-10.101427	-1.906002	3.651392	0.002168	0.710329
-9.198012	-1.965296	3.661389	0.002000	0.710531
-9.143629	-1.972693	3.671386	0.001990	0.710535
-9.307768	-1.942636	3.681382	0.002021	0.710536
-8.503851	-1.963264	3.691379	0.001872	0.710780
-8.537984	-1.910811	3.701376	0.001879	0.710872
-8.029548	-2.001195	3.711373	0.001784	0.710872
-8.361750	-1.942598	3.721370	0.001847	0.710870
-7.620172	-1.944809	3.731366	0.001709	0.711129
-7.557984	-1.952420	3.741363	0.001698	0.711135
-7.581865	-1.948532	3.751360	0.001702	0.711134
-7.186864	-1.939976	3.761357	0.001629	0.711290
-6.536006	-1.973270	3.771354	0.001508	0.711455
-6.724359	-1.939134	3.781350	0.001544	0.711455
-6.556260	-1.970671	3.791347	0.001513	0.711451
-6.255905	-1.874310	3.801344	0.001457	0.711750
-5.811489	-1.947989	3.811341	0.001375	0.711760
-6.059623	-1.902888	3.821338	0.001421	0.711761
-5.186771	-1.932116	3.831334	0.001259	0.712012
-4.715893	-1.976782	3.841331	0.001172	0.712090
-4.645841	-1.989750	3.851328	0.001159	0.712088
-4.555066	-2.006176	3.861325	0.001143	0.712087
-4.222980	-1.932863	3.871322	0.001081	0.712350
-3.785527	-1.993210	3.881318	0.001000	0.712384
-3.844039	-1.982329	3.891315	0.001011	0.712385
-3.759141	-1.962120	3.901312	0.000996	0.712454
-3.412399	-1.894839	3.911309	0.000932	0.712711
-3.258920	-1.921966	3.921306	0.000904	0.712710
-3.118551	-1.945815	3.931302	0.000878	0.712712
-2.844220	-1.845517	3.941299	0.000827	0.713008
-2.469713	-1.906017	3.951296	0.000758	0.713020
-2.344766	-1.927039	3.961293	0.000735	0.713022
-2.163541	-1.829294	3.971290	0.000701	0.713280
-2.074158	-1.804455	3.981286	0.000685	0.713360
-2.183834	-1.784891	3.991283	0.000706	0.713360
-1.974302	-1.678685	4.001280	0.000667	0.713645
-1.704585	-1.723140	4.011277	0.000617	0.713651
-1.481018	-1.685508	4.021274	0.000576	0.713804
-1.398299	-1.614545	4.031270	0.000561	0.713974
-1.321095	-1.607592	4.041267	0.000547	0.714014
-1.429656	-1.456224	4.051264	0.000567	0.714276
-1.007508	-1.523818	4.061261	0.000489	0.714291
-1.073669	-1.350552	4.071258	0.000502	0.714611
-0.961925	-1.351505	4.081254	0.000481	0.714648
-1.055427	-1.202466	4.091251	0.000499	0.714910
-1.213587	-1.107558	4.101248	0.000528	0.715041
-0.764785	-1.090672	4.111245	0.000445	0.715233
-0.670125	-0.980799	4.121242	0.000428	0.715484
-0.319428	-0.982755	4.131238	0.000363	0.715603
-0.448957	-0.814976	4.141235	0.000387	0.715889
-0.661135	-0.697499	4.151232	0.000427	0.716046
-0.536821	-0.631504	4.161229	0.000404	0.716220
-0.490666	-0.522325	4.171226	0.000396	0.716452
-0.416044	-0.386874	4.181222	0.000382	0.716746
-0.427556	-0.263821	4.191219	0.000385	0.716985
-0.388598	-0.145294	4.201216	0.000378	0.717232
-0.038510	-0.084632	4.211213	0.000313	0.717475
-0.083269	0.061742	4.221210	0.000321	0.717748
0.000000	0.250709	4.231206	0.000306	0.718150

-0.117856	0.897494	4.236211	0.000328	0.719385
0.091512	2.100838	4.241216	0.000288	0.721828
0.761260	3.828385	4.246221	0.000163	0.725448
0.861017	6.208147	4.251226	0.000143	0.730122
1.468428	9.013595	4.256230	0.000028	0.735761
1.832656	12.337738	4.261235	-0.000042	0.742267
2.286461	16.095619	4.266240	-0.000129	0.749568
2.658330	20.293376	4.271245	-0.000200	0.757595
3.102480	24.852336	4.276250	-0.000286	0.766231
3.702121	29.771322	4.281254	-0.000401	0.775480
4.280729	35.031475	4.286259	-0.000512	0.785229
4.775039	40.637521	4.291264	-0.000607	0.795449
5.246183	46.543600	4.296269	-0.000698	0.806060
5.364002	52.795562	4.301274	-0.000724	0.817025
6.003471	59.222912	4.306278	-0.000847	0.828303
6.878679	65.851402	4.311283	-0.001015	0.839840
7.317173	72.763636	4.316288	-0.001100	0.851564
8.185909	79.814419	4.321293	-0.001267	0.863481
10.408315	86.840265	4.326298	-0.001685	0.875581
10.930533	94.345524	4.331302	-0.001787	0.887803
11.625423	101.984759	4.336307	-0.001921	0.900117
12.059378	109.808434	4.341312	-0.002007	0.912481
12.903410	117.683410	4.346317	-0.002169	0.924868
13.708655	125.678796	4.351322	-0.002324	0.937262
14.535956	133.787434	4.356326	-0.002483	0.949669
15.279940	141.989852	4.361331	-0.002627	0.962033
16.003198	150.283542	4.366336	-0.002767	0.974367
16.558908	158.691617	4.371341	-0.002875	0.986668
17.391189	167.099904	4.376346	-0.003036	0.998887
18.021127	175.581377	4.381350	-0.003158	1.011010
18.837107	184.065265	4.386355	-0.003316	1.023038
19.571076	192.617715	4.391360	-0.003458	1.035000
20.349676	201.179585	4.396365	-0.003608	1.046848
20.868797	209.814058	4.401370	-0.003710	1.058600
21.526818	218.449464	4.406374	-0.003838	1.070256
22.681603	226.998186	4.411379	-0.004059	1.081784
23.076773	235.700924	4.416384	-0.004138	1.093221
23.934298	244.328755	4.421389	-0.004303	1.104544
24.655629	252.982363	4.426394	-0.004442	1.115755
25.287364	261.640882	4.431398	-0.004566	1.126842
25.902275	270.310951	4.436403	-0.004686	1.137830
26.622851	278.968740	4.441408	-0.004825	1.148721
27.371998	287.620391	4.446413	-0.004970	1.159507
28.013636	296.243248	4.451418	-0.005095	1.170136
28.747587	304.854337	4.456422	-0.005237	1.180674
29.103709	313.511685	4.461427	-0.005309	1.191096
29.846784	322.068296	4.466432	-0.005453	1.201387
30.617557	330.633919	4.471437	-0.005602	1.211607
31.102150	339.220304	4.476442	-0.005697	1.221708
31.854040	347.783422	4.481446	-0.005843	1.231751
32.260758	356.364033	4.486451	-0.005924	1.241666
32.717119	364.915852	4.491456	-0.006014	1.251479
33.448370	373.412895	4.496461	-0.006156	1.261207
33.957215	381.930990	4.501466	-0.006256	1.270841
34.553158	390.431927	4.506470	-0.006372	1.280399
35.279775	398.894468	4.511475	-0.006513	1.289869
35.997825	407.342968	4.516480	-0.006652	1.299252
36.337565	415.883993	4.521485	-0.006720	1.308599
36.733048	424.454159	4.526490	-0.006800	1.317921
37.517297	432.815114	4.531494	-0.006951	1.327023
38.155107	441.226691	4.536499	-0.007075	1.336091
38.670207	449.616623	4.541504	-0.007176	1.345053
39.292041	458.020124	4.546509	-0.007297	1.353988
39.956134	466.381165	4.551514	-0.007426	1.362827
40.439646	474.784783	4.556518	-0.007521	1.371622
41.010836	483.160193	4.561523	-0.007633	1.380347
41.623406	491.514759	4.566528	-0.007752	1.389003
42.214777	499.894253	4.571533	-0.007868	1.397626
42.582708	508.236492	4.576538	-0.007942	1.406122
42.945144	516.614053	4.581542	-0.008014	1.414601
43.434059	524.942283	4.586547	-0.008111	1.423000
43.902544	533.275793	4.591552	-0.008203	1.431352
44.518851	541.578693	4.596557	-0.008323	1.439650
44.939943	549.890814	4.601562	-0.008407	1.447877
45.494910	558.203997	4.606566	-0.008515	1.456080
46.178284	566.470739	4.611571	-0.008648	1.464212
46.619309	574.821281	4.616576	-0.008735	1.472341
47.073908	583.131624	4.621581	-0.008825	1.480390
47.340819	591.428580	4.626586	-0.008880	1.488352
48.113273	599.665830	4.631590	-0.009029	1.496294
48.487174	607.942562	4.636595	-0.009104	1.504169
48.695433	616.254757	4.641600	-0.009148	1.512011
49.266619	624.496255	4.646605	-0.009259	1.519802
49.665951	632.744333	4.651610	-0.009339	1.527533
50.022741	641.029496	4.656614	-0.009411	1.535253
50.509308	649.265952	4.661619	-0.009506	1.542909
50.945174	657.523155	4.666624	-0.009593	1.550538
51.871480	665.715629	4.671629	-0.009770	1.558143
51.956167	673.981351	4.676634	-0.009791	1.565653
52.308651	682.244903	4.681638	-0.009862	1.573165
52.595233	690.488012	4.686643	-0.009921	1.580613
53.215706	698.677781	4.691648	-0.010041	1.588027
53.993951	706.880867	4.696653	-0.010192	1.595440
54.637818	715.056888	4.701658	-0.010317	1.602776
54.949108	723.302883	4.706662	-0.010380	1.610092
55.337425	731.536318	4.711667	-0.010457	1.617375
55.885074	739.708107	4.716672	-0.010564	1.624594
56.259153	747.977918	4.721677	-0.010639	1.631842
56.673522	756.199074	4.726682	-0.010722	1.639021
57.484105	764.316334	4.731686	-0.010878	1.646134
57.970925	772.526301	4.736691	-0.010973	1.653250
58.136251	780.748906	4.741696	-0.011009	1.660304
58.721892	788.915496	4.746701	-0.011124	1.667336
59.364474	797.097507	4.751706	-0.011248	1.674360
59.959745	805.248739	4.756710	-0.011364	1.681322
60.299080	813.459124	4.761715	-0.011433	1.688270
60.563794	821.676679	4.766720	-0.011487	1.695186
61.006237	829.863295	4.771725	-0.011575	1.702072
61.459351	838.030850	4.776730	-0.011664	1.708915
62.081875	846.194199	4.781734	-0.011785	1.715749
62.529897	854.349507	4.786739	-0.011874	1.722527
62.725231	862.547397	4.791744	-0.011915	1.729280
63.275027	870.716609	4.796749	-0.012023	1.736029
63.931017	878.833005	4.801754	-0.012150	1.742722
64.300767	887.022235	4.806758	-0.012224	1.749413
64.772993	895.207273	4.811763	-0.012317	1.756087
65.156578	903.346488	4.816768	-0.012394	1.762687
65.435837	911.546538	4.821773	-0.012451	1.769299
65.739335	919.723695	4.826778	-0.012513	1.775871
66.275793	927.848891	4.831782	-0.012618	1.782405
66.783494	936.008927	4.836787	-0.012717	1.788940
66.992127	944.237794	4.841792	-0.012761	1.795469
67.459509	952.355880	4.846797	-0.012854	1.801918
68.390132	960.388020	4.851802	-0.013032	1.808333
68.803964	968.565241	4.856806	-0.013114	1.814776
69.466324	976.674786	4.861811	-0.013243	1.821173
69.846611	984.825945	4.866816	-0.013318	1.827546
70.470635	992.972276	4.871821	-0.013440	1.833922
70.658758	1001.135664	4.876826	-0.013480	1.840238
70.828173	1009.311650	4.881830	-0.013517	1.846539
71.213230	1017.474521	4.886835	-0.013593	1.852834
71.476417	1025.611859	4.891840	-0.013648	1.859073
71.947598	1033.735336	4.896845	-0.013740	1.865306
72.279151	1041.893735	4.901850	-0.013807	1.871528
72.595191	1050.034371	4.906854	-0.013871	1.877714
73.255856	1058.106063	4.911859	-0.013999	1.883867
73.641773	1066.228223	4.916864	-0.014076	1.890006
74.283785	1074.344738	4.921869	-0.014201	1.896150
74.584023	1082.466219	4.926874	-0.014262	1.902240
74.975541	1090.601025	4.931878	-0.014340	1.908330
75.413212	1098.749716	4.936883	-0.014427	1.914416
75.684171	1106.864200	4.941888	-0.014482	1.920438
76.119310	1114.985796	4.946893	-0.014568	1.926465
76.391312	1123.137369	4.951898	-0.014624	1.932478
76.831366	1131.248685	4.956902	-0.014711	1.938460
77.189667	1139.367958	4.961907	-0.014783	1.944421
77.433108	1147.518971	4.966912	-0.014834	1.950374
78.284170	1155.626009	4.971917	-0.014997	1.956343
78.714940	1163.706405	4.976922	-0.015082	1.962229
78.892995	1171.831668	4.981926	-0.015121	1.968102
79.190099	1179.980352	4.986931	-0.015181	1.973987
79.516918	1188.055989	4.991936	-0.015247	1.979806
79.462101	1196.219095	4.996941	-0.015242	1.985629
79.790926	1204.335236	5.001946	-0.015308	1.991443
80.466263	1212.378766	5.006950	-0.015439	1.997224
80.569492	1220.516269	5.011955	-0.015464	2.002995
80.638603	1228.635450	5.016960	-0.015482	2.008733
81.147956	1236.732543	5.021965	-0.015581	2.014485
81.299356	1244.838401	5.026970	-0.015615	2.020189
81.710020	1252.914977	5.031974	-0.015696	2.025884
82.147441	1261.041151	5.036979	-0.015783	2.031600
82.516536	1269.136171	5.041984	-0.015857	2.037271
82.941181	1277.203775	5.046989	-0.015941	2.042912
83.448459	1285.268808	5.051994	-0.016040	2.048545
83.749305	1293.409150	5.056998	-0.016102	2.054193
84.080395	1301.508902	5.062003	-0.016168	2.059801
84.152666	1309.623301	5.067008	-0.016187	2.065378
84.652051	1317.718352	5.072013	-0.016285	2.070969
84.934021	1325.823200	5.077018	-0.016343	2.076529
85.000568	1333.941434	5.082022	-0.016360	2.082063
85.246926	1342.041145	5.087027	-0.016411	2.087587
85.795274	1350.104814	5.092032	-0.016518	2.093102
85.839661	1358.238984	5.097037	-0.016532	2.098600
86.135302	1366.318704	5.102042	-0.016592	2.104072
86.407966	1374.421629	5.107046	-0.016648	2.109543
86.750242	1382.590803	5.112051	-0.016716	2.115050
86.773580	1390.662469	5.117056	-0.016726	2.120448
87.234297	1398.705093	5.122061	-0.016817	2.125854
87.579248	1406.772283	5.127066	-0.016886	2.131252
87.760260	1414.881632	5.132070	-0.016925	2.136648
87.906661	1422.976917	5.137075	-0.016957	2.142018
88.170598	1431.035546	5.142080	-0.017011	2.147362
88.439454	1439.159814	5.147085	-0.017067	2.152736
88.601877	1447.239603	5.152090	-0.017102	2.158057
88.893834	1455.295939	5.157094	-0.017161	2.163362
89.224987	1463.381524	5.162099	-0.017228	2.168677
89.331031	1471.493102	5.167104	-0.017253	2.173974
89.769955	1479.555149	5.172109	-0.017340	2.179258
90.197829	1487.605902	5.177114	-0.017425	2.184520
90.343397	1495.725816	5.182118	-0.017457	2.189788
90.570757	1503.853105	5.187123	-0.017504	2.195055
90.929570	1511.897077	5.192128	-0.017576	2.200268
91.204276	1519.962783	5.197133	-0.017632	2.205476
91.567210	1528.036551	5.202138	-0.017705	2.210684
92.062024	1536.084440	5.207142	-0.017802	2.215875
92.465937	1544.151117	5.212147	-0.017883	2.221057
92.355967	1552.285970	5.217152	-0.017867	2.226225
92.884145	1560.339655	5.222157	-0.017971	2.231386
93.085528	1568.440840	5.227162	-0.018013	2.236536
93.129989	1576.521962	5.232166	-0.018027	2.241648
93.402233	1584.598711	5.237171	-0.018082	2.246766
93.668731	1592.668554	5.242176	-0.018137	2.251866
94.120713	1600.734571	5.247181	-0.018226	2.256969
94.323717	1608.807117	5.252186	-0.018269	2.262043
94.723202	1616.869930	5.257190	-0.018349	2.267117
95.054114	1625.013231	5.262195	-0.018415	2.272223
95.136717	1633.113750	5.267200	-0.018436	2.277270
95.372174	1641.158072	5.272205	-0.018485	2.282283
95.592021	1649.210556	5.277210	-0.018531	2.287290
95.728655	1657.304448	5.282214	-0.018561	2.292304
96.103658	1665.367409	5.287219	-0.018636	2.297308
96.343473	1673.401529	5.292224	-0.018686	2.302272
96.604734	1681.483818	5.297229	-0.018740	2.307257
96.808957	1689.568891	5.302234	-0.018783	2.312227
97.290877	1697.608987	5.307238	-0.018878	2.317183
97.553265	1705.676134	5.312243	-0.018932	2.322126
97.596360	1713.752328	5.317248	-0.018945	2.327046
97.832097	1721.836649	5.322253	-0.018994	2.331977
98.266168	1729.887042	5.327258	-0.019080	2.336892
98.633962	1737.938379	5.332262	-0.019153	2.341793
99.008185	1746.005192	5.337267	-0.019228	2.346693
99.392453	1754.063125	5.342272	-0.019304	2.351578
99.783465	1762.155630	5.347277	-0.019382	2.356474
99.884573	1770.227281	5.352282	-0.019406	2.361324
100.044766	1778.290934	5.357286	-0.019441	2.366164
100.535061	1786.346647	5.362291	-0.019538	2.371016
100.656181	1794.430568	5.367296	-0.019565	2.375845
100.610815	1802.524490	5.372301	-0.019562	2.380657
100.943051	1810.575463	5.377306	-0.019629	2.385464
101.171936	1818.641447	5.382310	-0.019676	2.390262
101.312441	1826.740632	5.387315	-0.019708	2.395062
101.486889	1834.783070	5.392320	-0.019745	2.399823
101.670648	1842.841155	5.397325	-0.019785	2.404583
101.958186	1850.893290	5.402330	-0.019843	2.409339
102.139947	1858.983313	5.407334	-0.019882	2.414100
102.384634	1867.046126	5.412339	-0.019933	2.418840
102.543945	1875.081156	5.417344	-0.019967	2.423548
102.798178	1883.157943	5.422349	-0.020020	2.428278
103.164638	1891.277435	5.427354	-0.020093	2.433032
103.339947	1899.347098	5.432358	-0.020131	2.437734
103.610516	1907.367370	5.437363	-0.020186	2.442405
103.986334	1915.380698	5.442368	-0.020261	2.447071
104.189030	1923.469906	5.447373	-0.020304	2.451759
104.330420	1931.531825	5.452378	-0.020336	2.456418
104.479780	1939.573076	5.457382	-0.020369	2.461056
104.875628	1947.616148	5.462387	-0.020447	2.465705
104.889622	1955.696710	5.467392	-0.020455	2.470338
105.222674	1963.769168	5.472397	-0.020522	2.474982
105.459292	1971.796239	5.477402	-0.020571	2.479584
105.745583	1979.830554	5.482406	-0.020630	2.484185
106.141514	1987.890992	5.487411	-0.020708	2.488800
106.069426	1995.992078	5.492416	-0.020700	2.493396
106.565623	2004.036207	5.497421	-0.020798	2.497992
106.666788	2012.091552	5.502426	-0.020821	2.502557
106.741297	2020.157925	5.507430	-0.020840	2.507119
107.112283	2028.238276	5.512435	-0.020915	2.511701
107.508813	2036.277310	5.517440	-0.020993	2.516253
107.672425	2044.333806	5.522445	-0.021029	2.520791
107.980981	2052.359596	5.527450	-0.021091	2.525313
108.089882	2060.424133	5.532454	-0.021117	2.529834
108.558079	2068.477669	5.537459	-0.021209	2.534367
108.584532	2076.537018	5.542464	-0.021219	2.538864
109.079280	2084.559150	5.547469	-0.021316	2.543365
109.399526	2092.630379	5.552474	-0.021381	2.547872
109.504067	2100.705486	5.557478	-0.021406	2.552359
109.861371	2108.767049	5.562483	-0.021477	2.556848
110.125486	2116.784149	5.567488	-0.021531	2.561298
110.448579	2124.827724	5.572493	-0.021597	2.565759
110.419205	2132.929718	5.577498	-0.021596	2.570220
110.661894	2140.988756	5.582502	-0.021646	2.574669
111.036848	2149.028165	5.587507	-0.021721	2.579108
111.031447	2157.081274	5.592512	-0.021725	2.583520
111.275502	2165.142847	5.597517	-0.021776	2.587947
111.720619	2173.301048	5.602522	-0.021864	2.592433
111.724319	2181.421973	5.607526	-0.021870	2.596860
112.069477	2189.385238	5.612531	-0.021939	2.601218
112.187250	2197.396458	5.617536	-0.021966	2.605578
112.632555	2205.388469	5.622541	-0.022054	2.609943
112.933160	2213.453665	5.627546	-0.022115	2.614331
113.273296	2221.474517	5.632550	-0.022183	2.618690
113.546668	2229.526480	5.637555	-0.022239	2.623054
113.639714	2237.581275	5.642560	-0.022262	2.627400
113.983773	2245.635893	5.647565	-0.022331	2.631755
114.110845	2253.709006	5.652570	-0.022360	2.636099
114.004375	2261.762495	5.657574	-0.022345	2.640409
114.327287	2269.781268	5.662579	-0.022410	2.644722
114.583233	2277.819504	5.667584	-0.022463	2.649034
114.764528	2285.911477	5.672589	-0.022502	2.653363
114.872160	2293.966249	5.677594	-0.022527	2.657660
115.115349	2301.985254	5.682598	-0.022577	2.661940
115.458647	2310.040419	5.687603	-0.022646	2.666239
115.540404	2318.111164	5.692608	-0.022666	2.670522
115.786439	2326.177905	5.697613	-0.022717	2.674807
116.095727	2334.177907	5.702618	-0.022780	2.679053
116.391846	2342.200086	5.707622	-0.022840	2.683304
116.494779	2350.266842	5.712627	-0.022864	2.687559
116.686963	2358.316656	5.717632	-0.022905	2.691804
116.893574	2366.385889	5.722637	-0.022949	2.696053
116.975265	2374.415664	5.727642	-0.022969	2.700267
117.392763	2382.414688	5.732646	-0.023052	2.704480
117.545889	2390.497025	5.737651	-0.023085	2.708713
117.489892	2398.578228	5.742656	-0.023080	2.712925
117.848744	2406.607351	5.747661	-0.023152	2.717130
118.193933	2414.625526	5.752666	-0.023221	2.721321
118.324991	2422.663748	5.757670	-0.023251	2.725504
118.827990	2430.690014	5.762675	-0.023349	2.729696
119.228984	2438.756126	5.767680	-0.023429	2.733896
119.324414	2446.810686	5.772685	-0.023452	2.738066
119.529953	2454.847593	5.777690	-0.023495	2.742226
119.694608	2462.903482	5.782694	-0.023531	2.746387
119.934856	2470.974912	5.787699	-0.023581	2.750555
120.144853	2479.092702	5.792704	-0.023625	2.754738
120.555113	2487.078799	5.797709	-0.023707	2.758859
120.878649	2495.098854	5.802714	-0.023772	2.762987
121.077216	2503.119478	5.807718	-0.023814	2.767101
121.110068	2511.205208	5.812723	-0.023825	2.771232
121.188013	2519.255481	5.817728	-0.023845	2.775341
121.503176	2527.255694	5.822733	-0.023908	2.779433
121.742115	2535.297040	5.827738	-0.023958	2.783535
122.048470	2543.324703	5.832742	-0.024020	2.787629
122.245046	2551.410989	5.837747	-0.024062	2.791739
122.451817	2559.447637	5.842752	-0.024105	2.795819
122.675328	2567.473193	5.847757	-0.024152	2.799888
122.945115	2575.507068	5.852762	-0.024207	2.803958
123.102130	2583.541600	5.857766	-0.024242	2.808016
123.275962	2591.613852	5.862771	-0.024279	2.812088
123.552557	2599.641330	5.867776	-0.024336	2.816138
123.888477	2607.673096	5.872781	-0.024403	2.820187
124.071179	2615.699851	5.877786	-0.024442	2.824219
124.198294	2623.758905	5.882790	-0.024471	2.828258
124.582872	2631.833312	5.887795	-0.024548	2.832314
124.652508	2639.903424	5.892800	-0.024566	2.836344
124.954090	2647.906619	5.897805	-0.024627	2.840348
125.219218	2655.924164	5.902810	-0.024681	2.844351
125.368425	2663.973847	5.907814	-0.024714	2.848358
125.698632	2672.024547	5.912819	-0.024781	2.852371
125.846237	2680.067667	5.917824	-0.024813	2.856363
126.065167	2688.122294	5.922829	-0.024859	2.860359
126.210976	2696.147214	5.927834	-0.024891	2.864332
126.381858	2704.171676	5.932838	-0.024928	2.868299
126.814982	2712.238176	5.937843	-0.025014	2.872297
126.789195	2720.307223	5.942848	-0.025014	2.876265
127.074591	2728.327809	5.947853	-0.025072	2.880220
127.271573	2736.357987	5.952858	-0.025114	2.884170
127.384096	2744.383188	5.957862	-0.025140	2.888108
127.538906	2752.474735	5.962867	-0.025174	2.892074
127.677266	2760.513443	5.967872	-0.025205	2.896009
127.805203	2768.528459	5.972877	-0.025234	2.899926
128.200917	2776.531174	5.977882	-0.025313	2.903846
128.201483	2784.578293	5.982886	-0.025318	2.907762
128.582640	2792.679176	5.987891	-0.025394	2.911718
128.634694	2800.768921	5.992896	-0.025409	2.915646
128.941884	2808.726824	5.997901	-0.025471	2.919519
129.382673	2816.729229	6.002906	-0.025558	2.923415
129.473992	2824.749781	6.007910	-0.025580	2.927296
129.605967	2832.834846	6.012915	-0.025610	2.931205
129.514658	2840.911064	6.017920	-0.025598	2.935093
129.770089	2848.892695	6.022925	-0.025650	2.938948
130.236625	2856.904244	6.027930	-0.025742	2.942824
130.258972	2864.955934	6.032934	-0.025751	2.946690
130.995815	2872.958428	6.037939	-0.025894	2.950565
131.238900	2881.012826	6.042944	-0.025944	2.954434
131.389573	2889.070251	6.047949	-0.025977	2.958295
131.635709	2897.087447	6.052954	-0.026028	2.962136
131.822690	2905.104517	6.057958	-0.026068	2.965970
131.970899	2913.173610	6.062963	-0.026101	2.969821
132.071018	2921.243309	6.067968	-0.026124	2.973664
132.477360	2929.255912	6.072973	-0.026205	2.977492
132.469205	2937.313414	6.077978	-0.026209	2.981314
132.686955	2945.330819	6.082982	-0.026254	2.985124
133.007694	2953.380641	6.087987	-0.026319	2.988950
133.063759	2961.458474	6.092992	-0.026334	2.992771
133.260498	2969.513229	6.097997	-0.026376	2.996583
133.474661	2977.496328	6.103002	-0.026421	3.000357
133.631398	2985.479073	6.108006	-0.026455	3.004123
133.934008	2993.536270	6.113011	-0.026517	3.007927
133.893529	3001.600010	6.118016	-0.026514	3.011712
134.190103	3009.630501	6.123021	-0.026574	3.015494
134.210177	3017.684205	6.128026	-0.026583	3.019268
134.199695	3025.703127	6.133030	-0.026586	3.023019
134.633448	3033.728413	6.138035	-0.026672	3.026790
134.777433	3041.750631	6.143040	-0.026704	3.030541
134.883596	3049.800208	6.148045	-0.026729	3.034299
135.390294	3057.815555	6.153050	-0.026828	3.038055
135.362834	3065.860838	6.158054	-0.026828	3.041794
135.585093	3073.903638	6.163059	-0.026875	3.045540
135.665293	3081.942166	6.168064	-0.026895	3.049272
135.980408	3089.993358	6.173069	-0.026958	3.053017
136.132678	3098.043673	6.178074	-0.026992	3.056749
136.051004	3106.061680	6.183078	-0.026982	3.060451
136.750069	3114.034405	6.188083	-0.027117	3.064164
136.965439	3122.099159	6.193088	-0.027162	3.067892
137.035678	3130.202901	6.198093	-0.027180	3.071626
137.146777	3138.305593	6.203098	-0.027206	3.075358
137.169859	3146.270715	6.208102	-0.027215	3.079017
137.420536	3154.278069	6.213107	-0.027267	3.082703
137.464858	3162.305133	6.218112	-0.027280	3.086383
137.665103	3170.334917	6.223117	-0.027323	3.090067
137.869169	3178.380842	6.228122	-0.027366	3.093754
138.015713	3186.379324	6.233126	-0.027398	3.097413
138.192453	3194.455550	6.238131	-0.027436	3.101104
138.335289	3202.442709	6.243136	-0.027468	3.104749
138.480217	3210.487186	6.248141	-0.027500	3.108415
138.741654	3218.537849	6.253146	-0.027554	3.112086
139.021919	3226.579759	6.258150	-0.027611	3.115748
139.195496	3234.590221	6.263155	-0.027648	3.119388
138.955806	3242.631183	6.268160	-0.027609	3.123018
139.333008	3250.653372	6.273165	-0.027684	3.126663
139.699973	3258.681293	6.278170	-0.027757	3.130306
139.638233	3266.745176	6.283174	-0.027751	3.133942
140.157527	3274.758356	6.288179	-0.027853	3.137577
140.341035	3282.757228	6.293184	-0.027892	3.141186
140.456756	3290.789420	6.298189	-0.027918	3.144803
140.597683	3298.861839	6.303194	-0.027950	3.148434
140.818860	3306.895423	6.308198	-0.027996	3.152048
141.023062	3314.962308	6.313203	-0.028039	3.155672
141.263688	3322.929643	6.318208	-0.028089	3.159248
141.432950	3330.964075	6.323213	-0.028125	3.162848
141.528893	3339.010666	6.328218	-0.028148	3.166445
141.544240	3347.030147	6.333222	-0.028156	3.170023
141.930010	3355.078297	6.338227	-0.028233	3.173626
142.191145	3363.099379	6.343232	-0.028287	3.177207
142.515424	3371.110923	6.348237	-0.028352	3.180782
142.557395	3379.151021	6.353242	-0.028365	3.184354
142.774908	3387.191098	6.358246	-0.028411	3.187929
143.051600	3395.228309	6.363251	-0.028467	3.191502
143.031580	3403.300169	6.368256	-0.028469	3.195073
143.265308	3411.303179	6.373261	-0.028517	3.198620
143.435351	3419.335399	6.378266	-0.028554	3.202174
143.618069	3427.342851	6.383270	-0.028593	3.205714
143.881338	3435.382821	6.388275	-0.028647	3.209267
144.147272	3443.406033	6.393280	-0.028702	3.212809
144.384080	3451.453774	6.398285	-0.028751	3.216356
144.543145	3459.482269	6.403290	-0.028786	3.219888
144.599415	3467.486587	6.408294	-0.028801	3.223401
144.833622	3475.555005	6.413299	-0.028850	3.226946
144.871890	3483.586503	6.418304	-0.028862	3.230463
145.142152	3491.679440	6.423309	-0.028917	3.234012
145.339323	3499.681634	6.428314	-0.028959	3.237514
145.281803	3507.692632	6.433318	-0.028953	3.241007
145.470319	3515.686568	6.438323	-0.028994	3.244498
145.809526	3523.699667	6.443328	-0.029062	3.247999
145.952510	3531.738268	6.448333	-0.029093	3.251500
146.252243	3539.771886	6.453338	-0.029154	3.255002
146.348438	3547.787664	6.458342	-0.029177	3.258483
146.880856	3555.793666	6.463347	-0.029281	3.261974
146.891382	3563.824549	6.468352	-0.029288	3.265452
147.001828	3571.870764	6.473357	-0.029314	3.268936
147.134182	3579.959780	6.478362	-0.029344	3.272435
147.246940	3587.992717	6.483366	-0.029370	3.275906
147.484965	3595.984461	6.488371	-0.029419	3.279361
147.544698	3604.005981	6.493376	-0.029435	3.282818
147.774574	3612.039491	6.498381	-0.029483	3.286282
147.908308	3620.082273	6.503386	-0.029513	3.289744
147.975613	3628.111198	6.508390	-0.029531	3.293193
148.252618	3636.174908	6.513395	-0.029587	3.296662
148.553893	3644.142261	6.518400	-0.029649	3.300086
148.781820	3652.148689	6.523405	-0.029696	3.303521
149.210341	3660.212894	6.528410	-0.029781	3.306984
149.256763	3668.231275	6.533414	-0.029795	3.310410
149.401736	3676.334177	6.538419	-0.029827	3.313872
149.598759	3684.333996	6.543424	-0.029868	3.317289
149.509949	3692.351300	6.548429	-0.029857	3.320698
149.835592	3700.358594	6.553434	-0.029923	3.324116
149.635711	3708.384539	6.558438	-0.029890	3.327518
149.956360	3716.433964	6.563443	-0.029955	3.330946
150.270295	3724.444539	6.568448	-0.030019	3.334353
150.412496	3732.474799	6.573453	-0.030050	3.337759
150.615578	3740.536079	6.578458	-0.030093	3.341177
150.851569	3748.483862	6.583462	-0.030142	3.344545
150.922760	3756.573943	6.588467	-0.030160	3.347963
150.998911	3764.608955	6.593472	-0.030180	3.351355
151.309854	3772.654821	6.598477	-0.030243	3.354756
151.338716	3780.694023	6.603482	-0.030253	3.358141
151.492130	3788.690517	6.608486	-0.030287	3.361509
151.656025	3796.701646	6.613491	-0.030322	3.364880
151.713349	3804.726307	6.618496	-0.030338	3.368250
151.876244	3812.753734	6.623501	-0.030373	3.371621
152.200268	3820.815804	6.628506	-0.030439	3.375009
152.383260	3828.789889	6.633510	-0.030478	3.378352
152.407460	3836.866164	6.638515	-0.030487	3.381728
152.538015	3844.870448	6.643520	-0.030517	3.385075
152.940566	3852.880690	6.648525	-0.030597	3.388431
152.991870	3860.982669	6.653530	-0.030611	3.391809
153.258444	3869.040124	6.658534	-0.030666	3.395172
153.731348	3876.987736	6.663539	-0.030759	3.398494
153.944694	3884.998175	6.668544	-0.030804	3.401830
153.838759	3892.994355	6.673549	-0.030789	3.405145
154.004158	3901.047218	6.678554	-0.030825	3.408490
154.251592	3909.041685	6.683558	-0.030876	3.411810
154.405007	3917.109227	6.688563	-0.030910	3.415154
154.503252	3925.149282	6.693568	-0.030933	3.418481
155.006842	3933.128196	6.698573	-0.031032	3.421794
155.053121	3941.183809	6.703578	-0.031046	3.425120
155.200862	3949.188171	6.708582	-0.031078	3.428424
155.548854	3957.228654	6.713587	-0.031148	3.431747
155.600350	3965.290734	6.718592	-0.031163	3.435066
155.580343	3973.291247	6.723597	-0.031164	3.438354
155.901789	3981.337783	6.728602	-0.031229	3.441669
155.974197	3989.311965	6.733606	-0.031248	3.444943
156.144626	3997.365086	6.738611	-0.031284	3.448249
156.243967	4005.428719	6.743616	-0.031308	3.451554
156.524316	4013.446591	6.748621	-0.031365	3.454843
156.696560	4021.478647	6.753626	-0.031402	3.458131
156.848164	4029.491020	6.758630	-0.031436	3.461407
157.047809	4037.508746	6.763635	-0.031478	3.464684
157.177499	4045.558145	6.768640	-0.031507	3.467968
157.275318	4053.603972	6.773645	-0.031530	3.471247
157.693146	4061.658130	6.778650	-0.031613	3.474536
157.790965	4069.625583	6.783654	-0.031636	3.477777
158.019813	4077.675557	6.788659	-0.031684	3.481052
157.913342	4085.634156	6.793664	-0.031669	3.484277
158.244950	4093.677371	6.798669	-0.031736	3.487546
158.469559	4101.707377	6.803674	-0.031783	3.490804
158.341574	4109.753306	6.808678	-0.031764	3.494054
158.599238	4117.774222	6.813683	-0.031817	3.497303
158.864191	4125.759599	6.818688	-0.031872	3.500535
159.140425	4133.777939	6.823693	-0.031928	3.503778
159.410089	4141.832256	6.828698	-0.031983	3.507031
159.457587	4149.846195	6.833702	-0.031997	3.510259
159.515699	4157.934284	6.838707	-0.032013	3.513514
159.517226	4165.965079	6.843712	-0.032019	3.516741
159.891713	4173.898375	6.848717	-0.032093	3.519937
160.268136	4181.944824	6.853722	-0.032168	3.523176
160.394230	4189.962634	6.858726	-0.032197	3.526392
160.585812	4197.975037	6.863731	-0.032238	3.529606
160.702866	4206.090306	6.868736	-0.032265	3.532855
160.571319	4214.139717	6.873741	-0.032245	3.536068
160.687261	4222.123702	6.878746	-0.032272	3.539259
160.883657	4230.122979	6.883750	-0.032313	3.542455
161.218725	4238.158336	6.888755	-0.032381	3.545668
161.326217	4246.206446	6.893760	-0.032406	3.548875
161.466444	4254.257873	6.898765	-0.032437	3.552082
161.584612	4262.354445	6.903770	-0.032464	3.555303
161.716834	4270.301624	6.908774	-0.032494	3.558463
162.019207	4278.336992	6.913779	-0.032555	3.561659
162.104208	4286.309923	6.918784	-0.032576	3.564822
162.317937	4294.327007	6.923789	-0.032621	3.568003
162.593584	4302.363367	6.928794	-0.032677	3.571191
162.640273	4310.380402	6.933798	-0.032691	3.574361
162.696733	4318.427592	6.938803	-0.032707	3.577541
162.781373	4326.436378	6.943808	-0.032727	3.580703
162.968097	4334.436928	6.948813	-0.032767	3.583863
163.168267	4342.476955	6.953818	-0.032810	3.587035
163.302843	4350.470222	6.958822	-0.032840	3.590185
163.465509	4358.521767	6.963827	-0.032875	3.593355
163.788651	4366.551441	6.968832	-0.032940	3.596519
163.775904	4374.524955	6.973837	-0.032943	3.599648
163.798716	4382.578523	6.978842	-0.032952	3.602807
163.998652	4390.561937	6.983846	-0.032994	3.605940
164.234182	4398.615279	6.988851	-0.033043	3.609099
164.162777	4406.704810	6.993856	-0.033035	3.612261
164.470506	4414.688187	6.998861	-0.033097	3.615390
164.761474	4422.699809	7.003866	-0.033157	3.618526
164.781678	4430.724010	7.008870	-0.033166	3.621656
164.935578	4438.742558	7.013875	-0.033199	3.624786
165.117499	4446.764541	7.018880	-0.033238	3.627915
165.214817	4454.807485	7.023885	-0.033261	3.631047
165.567128	4462.879002	7.028890	-0.033332	3.634194
165.533387	4470.888847	7.033894	-0.033331	3.637304
165.813147	4478.887813	7.038899	-0.033388	3.640416
166.004726	4486.886161	7.043904	-0.033429	3.643522
166.003456	4494.915214	7.048909	-0.033433	3.646633
166.328279	4502.947252	7.053914	-0.033499	3.649750
166.284211	4511.003542	7.058918	-0.033496	3.652865
166.732578	4519.045132	7.063923	-0.033584	3.655984
167.093593	4527.014003	7.068928	-0.033657	3.659070
167.302978	4535.044615	7.073933	-0.033701	3.662173
167.310563	4543.099878	7.078938	-0.033707	3.665278
167.214811	4551.098408	7.083942	-0.033694	3.668356
167.678934	4559.144602	7.088947	-0.033786	3.671464
167.930360	4567.162573	7.093952	-0.033838	3.674553
167.848605	4575.181287	7.098957	-0.033828	3.677631
168.197292	4583.191748	7.103962	-0.033898	3.680714
168.353656	4591.168966	7.108966	-0.033932	3.683777
168.446947	4599.250836	7.113971	-0.033954	3.686876
168.751578	4607.258649	7.118976	-0.034016	3.689949
169.036347	4615.278674	7.123981	-0.034074	3.693024
169.138918	4623.310165	7.128986	-0.034098	3.696096
169.143561	4631.277939	7.133990	-0.034104	3.699139
169.309234	4639.342421	7.138995	-0.034140	3.702220
169.553036	4647.379107	7.144000	-0.034190	3.705290
169.438728	4655.398329	7.149005	-0.034174	3.708342
169.626899	4663.449614	7.154010	-0.034214	3.711411
169.928043	4671.521698	7.159014	-0.034275	3.714488
170.013525	4679.525753	7.164019	-0.034296	3.717531
170.162464	4687.506004	7.169024	-0.034329	3.720564
170.398793	4695.458418	7.174029	-0.034378	3.723587
170.516275	4703.533773	7.179034	-0.034405	3.726650
170.623204	4711.487852	7.184038	-0.034430	3.729665
170.862202	4719.598499	7.189043	-0.034480	3.732740
170.865938	4727.611898	7.194048	-0.034485	3.735770
170.849005	4735.609969	7.199053	-0.034487	3.738791
171.275777	4743.657727	7.204058	-0.034572	3.741839
171.385075	4751.593881	7.209062	-0.034597	3.744835
171.516379	4759.683411	7.214067	-0.034627	3.747887
171.496756	4767.739250	7.219072	-0.034628	3.750920
171.668244	4775.736596	7.224077	-0.034665	3.753933
171.921637	4783.776080	7.229082	-0.034717	3.756961
172.113267	4791.778594	7.234086	-0.034758	3.759972
172.315172	4799.794468	7.239091	-0.034801	3.762985
172.403640	4807.832156	7.244096	-0.034822	3.766002
172.487508	4815.848278	7.249101	-0.034843	3.769007
172.513223	4823.906921	7.254106	-0.034853	3.772026
172.568830	4831.920967	7.259110	-0.034868	3.775025
172.865888	4839.914247	7.264115	-0.034928	3.778020
173.155154	4847.955447	7.269120	-0.034987	3.781030
173.389889	4855.962960	7.274125	-0.035036	3.784024
173.648453	4864.007318	7.279130	-0.035089	3.787030
173.673274	4872.010992	7.284134	-0.035099	3.790013
173.919034	4880.060653	7.289139	-0.035150	3.793016
174.062647	4888.158978	7.294144	-0.035182	3.796032
173.937983	4896.098246	7.299149	-0.035163	3.798981
174.401180	4904.135866	7.304154	-0.035255	3.801977
174.466012	4912.055394	7.309158	-0.035272	3.804918
174.450218	4920.091078	7.314163	-0.035274	3.807898
174.671831	4928.112428	7.319168	-0.035320	3.810875
174.942125	4936.155029	7.324173	-0.035376	3.813859
175.026886	4944.219053	7.329178	-0.035397	3.816845
175.042881	4952.210631	7.334182	-0.035405	3.819800
175.152011	4960.202190	7.339187	-0.035430	3.822754
175.393310	4968.227919	7.344192	-0.035480	3.825722
175.580666	4976.227521	7.349197	-0.035520	3.828677
175.914911	4984.288553	7.354202	-0.035587	3.831655
175.860737	4992.331479	7.359206	-0.035582	3.834616
176.038728	5000.349609	7.364211	-0.035620	3.837570
176.164919	5008.339559	7.369216	-0.035649	3.840511
176.237514	5016.342965	7.374221	-0.035667	3.843453
176.523180	5024.379706	7.379226	-0.035726	3.846409
176.449597	5032.410515	7.384230	-0.035717	3.849354
176.580726	5040.445404	7.389235	-0.035746	3.852302
176.888517	5048.459641	7.394240	-0.035809	3.855244
176.772384	5056.483989	7.399245	-0.035792	3.858179
177.089836	5064.518657	7.404250	-0.035856	3.861124
177.386057	5072.526587	7.409254	-0.035917	3.864056
177.517406	5080.577137	7.414259	-0.035946	3.866999
177.449245	5088.615674	7.419264	-0.035939	3.869931
177.562830	5096.775455	7.424269	-0.035965	3.872908
178.048971	5104.863086	7.429274	-0.036060	3.875864
178.168683	5112.739267	7.434278	-0.036088	3.878734
178.404442	5120.730993	7.439283	-0.036137	3.881646
178.543018	5128.700531	7.444288	-0.036167	3.884546
178.746464	5136.702716	7.449293	-0.036210	3.887456
178.819645	5144.736859	7.454298	-0.036229	3.890374
178.931802	5152.776725	7.459302	-0.036255	3.893292
179.191922	5160.788144	7.464307	-0.036308	3.896200
179.177681	5168.810628	7.469312	-0.036311	3.899105
179.314658	5176.858779	7.474317	-0.036341	3.902020
179.563263	5184.818220	7.479322	-0.036393	3.904903
179.569749	5192.839479	7.484326	-0.036399	3.907802
179.766737	5200.849036	7.489331	-0.036441	3.910697
180.012945	5208.913149	7.494336	-0.036492	3.913611
180.077969	5216.931207	7.499341	-0.036509	3.916503
180.279568	5224.873666	7.504346	-0.036551	3.919368
180.381842	5232.956370	7.509350	-0.036575	3.922280
180.422634	5240.955362	7.514355	-0.036588	3.925158
180.604829	5248.985227	7.519360	-0.036627	3.928048
180.556138	5256.984930	7.524365	-0.036623	3.930920
181.014412	5265.044142	7.529370	-0.036713	3.933821
180.981664	5273.084484	7.534374	-0.036712	3.936705
181.194505	5281.026080	7.539379	-0.036757	3.939555
181.415482	5289.053349	7.544384	-0.036803	3.942433
181.346608	5297.063420	7.549389	-0.036795	3.945299
181.590967	5305.135446	7.554394	-0.036846	3.948190
181.703799	5313.150922	7.559398	-0.036872	3.951056
181.924379	5321.205481	7.564403	-0.036918	3.953936
182.041750	5329.237786	7.569408	-0.036945	3.956804
181.998687	5337.186546	7.574413	-0.036942	3.959638
182.508836	5345.200123	7.579418	-0.037042	3.962502
182.536749	5353.185064	7.584422	-0.037052	3.965346
182.399605	5361.250388	7.589427	-0.037032	3.968213
182.722776	5369.294223	7.594432	-0.037097	3.971078
182.868442	5377.292685	7.599437	-0.037129	3.973922
183.003280	5385.379271	7.604442	-0.037160	3.976795
182.943786	5393.318082	7.609446	-0.037153	3.979611
183.275391	5401.328680	7.614451	-0.037220	3.982456
183.351201	5409.397684	7.619456	-0.037239	3.985316
183.473546	5417.378601	7.624461	-0.037267	3.988143
183.714964	5425.433871	7.629466	-0.037317	3.990997
183.921935	5433.480706	7.634470	-0.037361	3.993845
184.014399	5441.518315	7.639475	-0.037383	3.996685
184.143657	5449.511340	7.644480	-0.037412	3.999509
184.262203	5457.530043	7.649485	-0.037439	4.002339
184.385599	5465.491351	7.654490	-0.037467	4.005148
184.331216	5473.560336	7.659494	-0.037462	4.007989
184.570764	5481.577419	7.664499	-0.037512	4.010815
184.659759	5489.644313	7.669504	-0.037534	4.013654
184.744693	5497.651392	7.674509	-0.037554	4.016469
184.977217	5505.669125	7.679514	-0.037603	4.019289
185.087951	5513.689091	7.684518	-0.037628	4.022106
185.279586	5521.648834	7.689523	-0.037669	4.024901
185.622741	5529.768824	7.694528	-0.037738	4.027752
185.532496	5537.721061	7.699533	-0.037726	4.030536
185.627419	5545.826858	7.704538	-0.037749	4.033374
185.767581	5553.859661	7.709542	-0.037780	4.036186
186.033302	5561.782810	7.714547	-0.037835	4.038959
186.241151	5569.866909	7.719552	-0.037879	4.041786
186.267405	5577.741719	7.724557	-0.037888	4.044535
186.435976	5585.835223	7.729562	-0.037925	4.047360
186.566548	5593.812417	7.734566	-0.037954	4.050143
186.561282	5601.852889	7.739571	-0.037958	4.052943
186.965213	5609.906881	7.744576	-0.038039	4.055752
187.123383	5617.888005	7.749581	-0.038073	4.058530
187.348484	5625.915916	7.754586	-0.038120	4.061324
187.422791	5633.901746	7.759590	-0.038139	4.064099
187.417112	5641.962948	7.764595	-0.038143	4.066897
187.656503	5649.942227	7.769600	-0.038193	4.069668
187.476245	5657.982915	7.774605	-0.038164	4.072452
187.959827	5666.008396	7.779610	-0.038259	4.075239
188.300870	5673.998422	7.784614	-0.038328	4.078010
188.347604	5681.995031	7.789619	-0.038341	4.080776
188.605448	5689.979609	7.794624	-0.038394	4.083540
188.657570	5698.064697	7.799629	-0.038409	4.086333
188.661570	5706.107494	7.804634	-0.038415	4.089110
188.584291	5714.142674	7.809638	-0.038406	4.091881
189.011706	5722.156225	7.814643	-0.038490	4.094649
189.383704	5730.149443	7.819648	-0.038565	4.097408
189.535880	5738.136791	7.824653	-0.038598	4.100159
189.639548	5746.176840	7.829658	-0.038622	4.102927
190.002222	5754.180611	7.834662	-0.038695	4.105683
189.834402	5762.219309	7.839667	-0.038669	4.108443
190.180211	5770.284728	7.844672	-0.038738	4.111216
190.340989	5778.318150	7.849677	-0.038773	4.113974
190.576203	5786.356965	7.854682	-0.038822	4.116734
190.588146	5794.297533	7.859686	-0.038829	4.119454
190.716563	5802.343911	7.864691	-0.038858	4.122211
190.910552	5810.342190	7.869696	-0.038899	4.124950
191.009211	5818.357612	7.874701	-0.038923	4.127693
191.344515	5826.374293	7.879706	-0.038990	4.130436
191.551187	5834.424011	7.884710	-0.039034	4.133188
191.662076	5842.436906	7.889715	-0.039060	4.135923
191.813685	5850.466510	7.894720	-0.039093	4.138664
191.969328	5858.481199	7.899725	-0.039127	4.141397
192.074119	5866.473728	7.904730	-0.039151	4.144120
191.959901	5874.527063	7.909734	-0.039135	4.146860
192.272911	5882.506308	7.914739	-0.039199	4.149577
192.570970	5890.602622	7.919744	-0.039259	4.152333
192.533178	5898.602176	7.924749	-0.039257	4.155050
192.648898	5906.631061	7.929754	-0.039284	4.157776
193.010164	5914.576688	7.934758	-0.039356	4.160476
193.222698	5922.576041	7.939763	-0.039401	4.163190
193.046757	5930.674188	7.944768	-0.039373	4.165932
193.019766	5938.619415	7.949773	-0.039373	4.168621
193.275022	5946.706996	7.954778	-0.039426	4.171361
193.295759	5954.724756	7.959782	-0.039435	4.174072
193.417765	5962.735118	7.964787	-0.039462	4.176780
193.651029	5970.728544	7.969792	-0.039511	4.179482
193.860974	5978.764108	7.974797	-0.039555	4.182195
194.007751	5986.725564	7.979802	-0.039587	4.184882
194.206072	5994.799868	7.984806	-0.039629	4.187605
194.333924	6002.828020	7.989811	-0.039658	4.190311
194.499888	6010.917720	7.994816	-0.039694	4.193035
194.657821	6018.933165	7.999821	-0.039729	4.195733
194.880002	6026.878396	8.004826	-0.039775	4.198406
194.769895	6034.909961	8.009830	-0.039759	4.201103
194.974348	6042.864191	8.014835	-0.039803	4.203775
195.359300	6050.902640	8.019840	-0.039879	4.206476
195.477180	6058.871816	8.024845	-0.039906	4.209149
195.620992	6066.939452	8.029850	-0.039938	4.211854
195.639940	6074.948085	8.034854	-0.039947	4.214535
195.785399	6083.005574	8.039859	-0.039979	4.217233
195.992242	6090.965571	8.044864	-0.040022	4.219897
196.078990	6099.004388	8.049869	-0.040044	4.222585
196.486517	6106.989219	8.054874	-0.040125	4.225255
196.483926	6115.073798	8.059878	-0.040129	4.227954
196.331159	6123.055627	8.064883	-0.040106	4.230615
196.762156	6131.101197	8.069888	-0.040191	4.233301
196.777414	6139.086359	8.074893	-0.040199	4.235961
196.891631	6147.099018	8.079898	-0.040225	4.238630
197.080716	6155.139972	8.084902	-0.040265	4.241307
197.207380	6163.069528	8.089907	-0.040294	4.243945
197.383446	6171.177484	8.094912	-0.040332	4.246641
197.437498	6179.141756	8.099917	-0.040347	4.249286
197.845367	6187.185820	8.104922	-0.040428	4.251959
197.933551	6195.226104	8.109926	-0.040450	4.254627
197.971887	6203.268140	8.114931	-0.040462	4.257292
198.208464	6211.280586	8.119936	-0.040511	4.259949
198.424710	6219.252462	8.124941	-0.040556	4.262590
198.549835	6227.314906	8.129946	-0.040584	4.265258
198.672611	6235.340958	8.134950	-0.040612	4.267913
198.834267	6243.325662	8.139955	-0.040648	4.270552
199.017772	6251.430186	8.144960	-0.040687	4.273230
198.960753	6259.440185	8.149965	-0.040681	4.275873
199.135047	6267.429221	8.154970	-0.040719	4.278509
199.308927	6275.431800	8.159974	-0.040756	4.281148
199.358164	6283.420781	8.164979	-0.040770	4.283780
199.564394	6291.465736	8.169984	-0.040814	4.286430
199.646525	6299.435352	8.174989	-0.040834	4.289052
199.744753	6307.513971	8.179994	-0.040857	4.291709
199.825784	6315.513477	8.184998	-0.040878	4.294338
200.144899	6323.559611	8.190003	-0.040942	4.296983
200.244076	6331.546745	8.195008	-0.040966	4.299605
200.112849	6339.583433	8.200013	-0.040946	4.302239
200.427057	6347.553300	8.205018	-0.041010	4.304854
200.556235	6355.640299	8.210022	-0.041039	4.307504
200.479424	6363.590300	8.215027	-0.041030	4.310106
200.660561	6371.660253	8.220032	-0.041068	4.312747
200.815917	6379.670884	8.225037	-0.041102	4.315368
200.909339	6387.659212	8.230042	-0.041125	4.317979
200.943218	6395.683429	8.235046	-0.041136	4.320599
201.264680	6403.646679	8.240051	-0.041201	4.323200
201.337648	6411.685566	8.245056	-0.041220	4.325823
201.325144	6419.716904	8.250061	-0.041222	4.328441
201.539637	6427.736580	8.255066	-0.041267	4.331055
201.866154	6435.812457	8.260070	-0.041333	4.333686
202.002757	6443.817842	8.265075	-0.041364	4.336292
202.251481	6451.818007	8.270080	-0.041415	4.338895
202.338371	6459.801550	8.275085	-0.041436	4.341490
202.350957	6467.846294	8.280090	-0.041444	4.344103
202.359367	6475.868078	8.285094	-0.041450	4.346707
202.492512	6483.854547	8.290099	-0.041480	4.349298
202.703911	6491.942488	8.295104	-0.041525	4.351922
202.796186	6499.974211	8.300109	-0.041547	4.354524
202.995679	6507.968113	8.305114	-0.041589	4.357114
203.030510	6515.903559	8.310118	-0.041600	4.359682
203.038406	6523.956251	8.315123	-0.041607	4.362287
203.195999	6531.915178	8.320128	-0.041641	4.364860
203.335031	6539.952707	8.325133	-0.041672	4.367457
203.381818	6548.020072	8.330138	-0.041686	4.370062
203.592701	6556.049470	8.335142	-0.041730	4.372654
203.784695	6563.963016	8.340147	-0.041771	4.375207
203.974408	6572.052838	8.345152	-0.041812	4.377815
203.978090	6580.040453	8.350157	-0.041817	4.380387
204.047249	6588.063597	8.355162	-0.041835	4.382970
204.345374	6596.069902	8.360166	-0.041896	4.385547
204.296153	6604.094042	8.365171	-0.041892	4.388127
204.412541	6612.137463	8.370176	-0.041918	4.390712
204.691014	6620.148810	8.375181	-0.041975	4.393286
204.698329	6628.172574	8.380186	-0.041982	4.395861
204.672719	6636.190904	8.385190	-0.041982	4.398433
204.967549	6644.195851	8.390195	-0.042042	4.401000
205.001889	6652.185572	8.395200	-0.042053	4.403560
204.999582	6660.207878	8.400205	-0.042058	4.406128
205.213226	6668.207929	8.405210	-0.042103	4.408689
205.609217	6676.288890	8.410214	-0.042182	4.411276
205.551055	6684.295993	8.415219	-0.042176	4.413834
205.785577	6692.379390	8.420224	-0.042225	4.416418
206.185202	6700.334950	8.425229	-0.042304	4.418959
206.215049	6708.350840	8.430234	-0.042315	4.421517
206.346386	6716.341453	8.435238	-0.042344	4.424065
206.276718	6724.383833	8.440243	-0.042336	4.426628
206.440877	6732.435251	8.445248	-0.042372	4.429193
206.369735	6740.412417	8.450253	-0.042364	4.431732
206.594396	6748.472354	8.455258	-0.042411	4.434297
206.798436	6756.529488	8.460262	-0.042454	4.436859
207.002469	6764.453774	8.465267	-0.042497	4.439378
207.163120	6772.516002	8.470272	-0.042532	4.441939
207.172932	6780.455117	8.475277	-0.042538	4.444459
207.387746	6788.528918	8.480282	-0.042583	4.447021
207.577704	6796.515196	8.485286	-0.042624	4.449553
207.604965	6804.547646	8.490291	-0.042634	4.452098
207.699060	6812.628235	8.495296	-0.042657	4.454657
207.567109	6820.591040	8.500301	-0.042637	4.457177
207.841395	6828.567090	8.505306	-0.042693	4.459701
208.075523	6836.643104	8.510310	-0.042742	4.462254
208.024703	6844.603708	8.515315	-0.042737	4.464769
208.290816	6852.676803	8.520320	-0.042792	4.467319
208.612122	6860.632259	8.525325	-0.042857	4.469831
208.866868	6868.715868	8.530330	-0.042909	4.472381
208.913588	6876.716377	8.535334	-0.042923	4.474903
208.958858	6884.708554	8.540339	-0.042937	4.477421
209.283107	6892.691319	8.545344	-0.043002	4.479936
209.397240	6900.716669	8.550349	-0.043028	4.482461
209.414911	6908.734698	8.555354	-0.043037	4.484983
209.392558	6916.784491	8.560359	-0.043038	4.487513
209.528394	6924.780567	8.565363	-0.043068	4.490025
209.672828	6932.842769	8.570368	-0.043100	4.492557
209.929544	6940.838828	8.575373	-0.043153	4.495067
210.052538	6948.832766	8.580378	-0.043181	4.497574
210.025666	6956.863500	8.585383	-0.043181	4.500091
209.955218	6964.874201	8.590387	-0.043173	4.502600
210.458413	6972.876263	8.595392	-0.043271	4.505107
210.274388	6980.903941	8.600397	-0.043242	4.507618
210.473867	6988.905805	8.605402	-0.043284	4.510121
210.969482	6997.003658	8.610407	-0.043382	4.512653
211.088638	7005.001349	8.615411	-0.043409	4.515152
210.875450	7013.034167	8.620416	-0.043374	4.517659
211.006575	7020.946605	8.625421	-0.043404	4.520128
211.230241	7028.957863	8.630426	-0.043450	4.522627
211.313861	7036.969666	8.635431	-0.043471	4.525124
211.438706	7044.988647	8.640435	-0.043499	4.527623
211.540004	7053.017293	8.645440	-0.043523	4.530122
211.665941	7061.057279	8.650445	-0.043552	4.532624
211.674333	7069.095508	8.655450	-0.043558	4.535124
212.003353	7077.111020	8.660455	-0.043625	4.537616
212.473582	7085.081948	8.665459	-0.043717	4.540093
212.544520	7093.098033	8.670464	-0.043735	4.542582
212.588879	7101.073414	8.675469	-0.043749	4.545057
212.819349	7109.120599	8.680474	-0.043797	4.547553
212.820874	7117.185630	8.685479	-0.043802	4.550053
213.072569	7125.190293	8.690483	-0.043854	4.552533
213.400900	7133.234345	8.695488	-0.043920	4.555024
213.357598	7141.262524	8.700493	-0.043917	4.557508
213.509592	7149.204304	8.705498	-0.043950	4.559964
213.527493	7157.227809	8.710503	-0.043959	4.562445
213.617025	7165.204848	8.715507	-0.043981	4.564909
213.813043	7173.285939	8.720512	-0.044022	4.567404
213.799782	7181.264059	8.725517	-0.044025	4.569866
214.045183	7189.326539	8.730522	-0.044075	4.572353
214.090278	7197.380022	8.735527	-0.044089	4.574836
214.041942	7205.364216	8.740531	-0.044085	4.577296
214.278687	7213.358918	8.745536	-0.044134	4.579758
214.339061	7221.387955	8.750541	-0.044150	4.582229
214.303904	7229.338362	8.755546	-0.044149	4.584674
214.570237	7237.438533	8.760551	-0.044204	4.587165
214.697162	7245.375839	8.765555	-0.044232	4.589604
214.990493	7253.513337	8.770560	-0.044292	4.592103
215.110525	7261.511240	8.775565	-0.044319	4.594558
215.151926	7269.530915	8.780570	-0.044332	4.597018
215.230123	7277.475406	8.785575	-0.044352	4.599454
215.278973	7285.518961	8.790579	-0.044366	4.601919
215.616857	7293.498214	8.795584	-0.044434	4.604362
215.891366	7301.560460	8.800589	-0.044490	4.606830
215.674172	7309.521345	8.805594	-0.044454	4.609266
215.919680	7317.628074	8.810599	-0.044505	4.611745
216.109973	7325.597252	8.815603	-0.044546	4.614180
216.205080	7333.650481	8.820608	-0.044569	4.616640
216.210916	7341.595523	8.825613	-0.044575	4.619065
216.343781	7349.692161	8.830618	-0.044604	4.621536
216.827744	7357.649980	8.835623	-0.044700	4.623963
216.704183	7365.655848	8.840627	-0.044682	4.626403
216.746492	7373.674240	8.845632	-0.044695	4.628845
216.927642	7381.710366	8.850637	-0.044733	4.631292
216.924171	7389.732125	8.855642	-0.044738	4.633733
217.045693	7397.798338	8.860647	-0.044765	4.636187
217.234571	7405.737494	8.865651	-0.044806	4.638600
217.465130	7413.781666	8.870656	-0.044854	4.641044
217.504866	7421.734156	8.875661	-0.044866	4.643459
217.742852	7429.804423	8.880666	-0.044915	4.645908
217.758352	7437.817781	8.885671	-0.044923	4.648339
217.802983	7445.831301	8.890675	-0.044937	4.650768
218.220462	7453.899536	8.895680	-0.045019	4.653213
218.282893	7461.894829	8.900685	-0.045036	4.655634
218.222483	7469.867106	8.905690	-0.045030	4.658047
218.374670	7477.877243	8.910695	-0.045063	4.660471
218.530088	7485.862711	8.915699	-0.045097	4.662885
218.832353	7493.973826	8.920704	-0.045159	4.665336
218.849089	7501.963118	8.925709	-0.045167	4.667750
218.987500	7509.949820	8.930714	-0.045198	4.670161
219.232853	7518.026033	8.935719	-0.045248	4.672598
219.301044	7526.097481	8.940723	-0.045266	4.675032
219.419692	7534.109178	8.945728	-0.045293	4.677447
219.643391	7541.994983	8.950733	-0.045340	4.679822
219.658095	7550.025897	8.955738	-0.045348	4.682240
219.817469	7557.996374	8.960743	-0.045382	4.684639
219.722024	7566.038121	8.965747	-0.045370	4.687058
220.019561	7574.040527	8.970752	-0.045430	4.689464
220.099499	7582.086414	8.975757	-0.045450	4.691882
220.354448	7590.078287	8.980762	-0.045503	4.694281
220.449172	7598.151372	8.985767	-0.045525	4.696705
220.153876	7606.076274	8.990771	-0.045475	4.699083
220.468059	7614.158051	8.995776	-0.045539	4.701506
220.743334	7622.113626	9.000781	-0.045595	4.703890
220.724668	7630.165096	9.005786	-0.045597	4.706302
220.977200	7638.166341	9.010791	-0.045649	4.708697
221.228047	7646.199926	9.015795	-0.045701	4.711101
221.239195	7654.258858	9.020800	-0.045708	4.713511
221.026209	7662.282570	9.025805	-0.045673	4.715911
221.366438	7670.213355	9.030810	-0.045741	4.718280
221.707546	7678.274792	9.035815	-0.045810	4.720686
221.655176	7686.277542	9.040819	-0.045805	4.723075
221.675388	7694.306936	9.045824	-0.045814	4.725471
221.880036	7702.313767	9.050829	-0.045857	4.727858
221.964540	7710.335176	9.055834	-0.045878	4.730248
221.863562	7718.408249	9.060839	-0.045864	4.732654
222.039441	7726.341159	9.065843	-0.045902	4.735015
222.320515	7734.451205	9.070848	-0.045960	4.737428
222.317721	7742.376897	9.075853	-0.045964	4.739785
222.449129	7750.425525	9.080858	-0.045994	4.742178
222.905427	7758.413263	9.085863	-0.046084	4.744550
222.850453	7766.404095	9.090867	-0.046078	4.746923
222.792349	7774.473572	9.095872	-0.046073	4.749319
222.866834	7782.498010	9.100877	-0.046092	4.751699
222.929648	7790.533753	9.105882	-0.046108	4.754082
223.161006	7798.589131	9.110887	-0.046156	4.756469
223.463310	7806.501876	9.115891	-0.046218	4.758812
223.703405	7814.576127	9.120896	-0.046268	4.761202
223.615974	7822.506134	9.125901	-0.046256	4.763549
223.622198	7830.549882	9.130906	-0.046262	4.765928
223.914073	7838.597948	9.135911	-0.046322	4.768306
223.891729	7846.570198	9.140915	-0.046323	4.770662
223.944042	7854.664682	9.145920	-0.046338	4.773053
223.959610	7862.635845	9.150925	-0.046346	4.775406
224.269162	7870.648607	9.155930	-0.046408	4.777769
224.389964	7878.666170	9.160935	-0.046436	4.780133
224.348445	7886.667593	9.165939	-0.046433	4.782491
224.627404	7894.663492	9.170944	-0.046490	4.784846
224.940953	7902.716940	9.175949	-0.046553	4.787216
224.930038	7910.687253	9.180954	-0.046556	4.789562
225.199361	7918.778999	9.185959	-0.046612	4.791941
225.227969	7926.782235	9.190963	-0.046622	4.794294
225.383790	7934.787007	9.195968	-0.046656	4.796646
225.748316	7942.744609	9.200973	-0.046729	4.798982
225.821814	7950.766802	9.205978	-0.046748	4.801337
225.857058	7958.797716	9.210983	-0.046759	4.803694
226.021397	7966.764288	9.215987	-0.046795	4.806029
226.242252	7974.841134	9.220992	-0.046841	4.808396
226.337666	7982.851886	9.225997	-0.046864	4.810743
226.370243	7990.259968	9.231002	-0.046875	4.812913
226.588706	7994.836077	9.236007	-0.046918	4.814251

226.657074	7997.392776	9.241011	-0.046932	4.814999
226.696490	7998.737495	9.246016	-0.046940	4.815393
226.660601	7999.209502	9.251021	-0.046934	4.815531
226.892056	8000.163763	9.256026	-0.046977	4.815809
226.930940	8000.185709	9.261031	-0.046985	4.815815
226.861287	8000.162173	9.266035	-0.046971	4.815809
227.043970	8000.162952	9.271040	-0.047005	4.815808
227.057687	8000.152488	9.276045	-0.047008	4.815805
227.082044	8000.163532	9.281050	-0.047012	4.815808
227.166313	8000.153132	9.286055	-0.047027	4.815805
227.172451	8000.137211	9.291059	-0.047028	4.815800
227.194772	8000.168494	9.296064	-0.047032	4.815809
227.246508	8000.178910	9.301069	-0.047042	4.815812
227.292623	8000.178568	9.306074	-0.047050	4.815812
227.335059	8000.173898	9.311079	-0.047058	4.815810
227.166255	8000.162642	9.316083	-0.047026	4.815808
227.357819	8000.200905	9.321088	-0.047062	4.815818
227.528825	8000.162022	9.326093	-0.047094	4.815806
227.496147	8000.188156	9.331098	-0.047087	4.815813
227.474139	8000.189922	9.336103	-0.047083	4.815814
227.606359	8000.154685	9.341107	-0.047107	4.815803
227.511584	8000.183023	9.346112	-0.047090	4.815812
227.523291	8000.140519	9.351117	-0.047092	4.815799
227.672921	8000.161041	9.356122	-0.047119	4.815805
227.703239	8000.160445	9.361127	-0.047125	4.815804
227.491629	8000.126097	9.366131	-0.047085	4.815795
227.541124	8000.193023	9.371136	-0.047094	4.815815
227.476295	8000.161028	9.376141	-0.047082	4.815806
227.600129	8000.171534	9.381146	-0.047105	4.815808
227.895211	8000.199722	9.386151	-0.047160	4.815815
227.749864	8000.178172	9.391155	-0.047132	4.815809
227.725966	8000.173506	9.396160	-0.047128	4.815808
227.849534	8000.147732	9.401165	-0.047151	4.815800
227.923096	8000.179837	9.406170	-0.047164	4.815809
227.916012	8000.161570	9.411175	-0.047163	4.815804
227.852916	8000.173347	9.416179	-0.047151	4.815808
227.999160	8000.210885	9.421184	-0.047178	4.815818
228.161125	8000.187861	9.426189	-0.047208	4.815810
227.961113	8000.208110	9.431194	-0.047170	4.815817
227.904158	8000.201847	9.436199	-0.047160	4.815816
228.140563	8000.160812	9.441203	-0.047203	4.815803
227.986617	8000.223411	9.446208	-0.047175	4.815822
228.042113	8000.169872	9.451213	-0.047185	4.815806
227.958707	8000.175988	9.456218	-0.047169	4.815808
228.206081	8000.174605	9.461223	-0.047215	4.815806
228.027988	8000.152530	9.466227	-0.047182	4.815801
228.196297	8000.203225	9.471232	-0.047213	4.815815
228.374321	8000.195396	9.476237	-0.047246	4.815812
227.973659	8000.184687	9.481242	-0.047171	4.815810
228.081168	8000.181062	9.486247	-0.047191	4.815809
227.878660	8000.173531	9.491251	-0.047153	4.815808
227.958244	8000.191863	9.496256	-0.047168	4.815813
227.976807	8000.181476	9.501261	-0.047171	4.815809
228.182008	8000.178350	9.506266	-0.047209	4.815808
228.329931	8000.184975	9.511271	-0.047236	4.815809
228.162755	8000.157740	9.516275	-0.047205	4.815802
228.273636	8000.208581	9.521280	-0.047225	4.815816
228.297555	8000.187611	9.526285	-0.047230	4.815810
228.145285	8000.190488	9.531290	-0.047201	4.815811
228.278227	8000.210743	9.536295	-0.047226	4.815817
228.396424	8000.155009	9.541299	-0.047247	4.815800
228.412080	8000.204324	9.546304	-0.047250	4.815814
228.210253	8000.181867	9.551309	-0.047212	4.815808
228.332822	8000.179550	9.556314	-0.047235	4.815807
228.629712	8000.230175	9.561319	-0.047290	4.815821
228.163442	8000.169335	9.566323	-0.047203	4.815805
228.197522	8000.209342	9.571328	-0.047209	4.815817
228.223315	8000.221477	9.576333	-0.047214	4.815820
228.211094	8000.204195	9.581338	-0.047212	4.815815
228.259297	8000.198551	9.586343	-0.047220	4.815813
228.247992	8000.188752	9.591347	-0.047218	4.815810
228.383289	8000.232517	9.596352	-0.047243	4.815823
228.252563	8000.187728	9.601357	-0.047219	4.815810
228.256991	8000.173914	9.606362	-0.047219	4.815806
228.534997	8000.215700	9.611367	-0.047271	4.815817
228.422820	8000.193614	9.616371	-0.047250	4.815811
228.606723	8000.227490	9.621376	-0.047284	4.815820
228.701264	8000.178845	9.626381	-0.047301	4.815805
228.553736	8000.211672	9.631386	-0.047274	4.815816
228.525235	8000.204798	9.636391	-0.047268	4.815814
228.511157	8000.231231	9.641395	-0.047265	4.815822
228.583745	8000.197171	9.646400	-0.047279	4.815811
228.738214	8000.212437	9.651405	-0.047307	4.815815
228.297820	8000.191488	9.656410	-0.047225	4.815811
228.664861	8000.184556	9.661415	-0.047293	4.815807
228.576810	8000.140452	9.666419	-0.047277	4.815795
228.674560	8000.178280	9.671424	-0.047295	4.815805
228.543718	8000.181501	9.676429	-0.047270	4.815807
228.607146	8000.204908	9.681434	-0.047282	4.815813
228.771768	8000.223538	9.686439	-0.047312	4.815818
228.657382	8000.203550	9.691443	-0.047291	4.815813
228.725473	8000.212096	9.696448	-0.047303	4.815815
228.755244	8000.188018	9.701453	-0.047309	4.815808
228.536636	8000.206902	9.706458	-0.047268	4.815814
228.662607	8000.228112	9.711463	-0.047291	4.815820
228.721019	8000.194892	9.716467	-0.047302	4.815810
228.593228	8000.217367	9.721472	-0.047278	4.815817
228.604236	8000.195123	9.726477	-0.047280	4.815811
228.766357	8000.172101	9.731482	-0.047310	4.815803
228.541204	8000.204750	9.736487	-0.047268	4.815814
228.471955	8000.170550	9.741491	-0.047255	4.815804
228.820577	8000.186796	9.746496	-0.047319	4.815807
228.677011	8000.180210	9.751501	-0.047292	4.815806
228.367650	8000.199772	9.756506	-0.047235	4.815813
228.715710	8000.204273	9.761511	-0.047299	4.815813
228.861396	8000.221532	9.766515	-0.047326	4.815817
228.678303	8000.220713	9.771520	-0.047292	4.815818
228.877561	8000.208957	9.776525	-0.047329	4.815813
228.767767	8000.149566	9.781530	-0.047308	4.815797
228.824903	8000.181409	9.786535	-0.047319	4.815806
228.694186	8000.171828	9.791539	-0.047294	4.815803
228.863493	8000.221474	9.796544	-0.047326	4.815817
228.819948	8000.186618	9.801549	-0.047317	4.815807
228.737732	8000.204489	9.806554	-0.047302	4.815813
228.811380	8000.226994	9.811559	-0.047315	4.815819
228.744302	8000.223769	9.816563	-0.047303	4.815818
228.719142	8000.220149	9.821568	-0.047298	4.815818
228.618293	8000.209981	9.826573	-0.047279	4.815815
228.797394	8000.193634	9.831578	-0.047312	4.815809
228.782474	8000.236057	9.836583	-0.047309	4.815822
228.713555	8000.212530	9.841587	-0.047296	4.815815
228.830551	8000.207990	9.846592	-0.047318	4.815813
228.730933	8000.190373	9.851597	-0.047299	4.815809
228.768100	8000.216561	9.856602	-0.047306	4.815816
228.811565	8000.232180	9.861607	-0.047314	4.815821
228.910212	8000.215609	9.866611	-0.047332	4.815815
228.832210	8000.197272	9.871616	-0.047317	4.815810
228.950740	8000.173551	9.876621	-0.047339	4.815803
228.964510	8000.200430	9.881626	-0.047341	4.815811
229.151778	8000.246097	9.886631	-0.047376	4.815823
228.864612	8000.241475	9.891635	-0.047322	4.815823
228.933822	8000.229767	9.896640	-0.047335	4.815819
228.884726	8000.216161	9.901645	-0.047326	4.815816
229.018290	8000.231092	9.906650	-0.047350	4.815819
229.170408	8000.236718	9.911655	-0.047379	4.815820
229.051303	8000.217721	9.916659	-0.047356	4.815815
228.877855	8000.223458	9.921664	-0.047324	4.815818
228.895217	8000.234391	9.926669	-0.047327	4.815821
228.912175	8000.226112	9.931674	-0.047330	4.815818
229.014808	8000.260819	9.936679	-0.047349	4.815828
228.808534	8000.198813	9.941683	-0.047310	4.815811
228.948468	8000.212779	9.946688	-0.047336	4.815814
229.093251	8000.210818	9.951693	-0.047363	4.815813
228.923254	8000.241151	9.956698	-0.047331	4.815823
229.103695	8000.238696	9.961703	-0.047364	4.815821
229.124514	8000.182467	9.966707	-0.047368	4.815805
229.059888	8000.219825	9.971712	-0.047356	4.815816
229.061124	8000.197424	9.976717	-0.047356	4.815809
228.918045	8000.194046	9.981722	-0.047329	4.815809
229.114691	8000.217458	9.986727	-0.047366	4.815815
228.878201	8000.188042	9.991731	-0.047321	4.815808
228.875976	8000.211464	9.996736	-0.047321	4.815814
229.064377	8000.195266	10.001741	-0.047356	4.815809
229.163941	8000.163773	10.006746	-0.047374	4.815799
229.116462	8000.219544	10.011751	-0.047365	4.815816
228.978701	8000.171440	10.016755	-0.047339	4.815802
228.935792	8000.209146	10.021760	-0.047331	4.815813
229.041639	8000.223633	10.026765	-0.047351	4.815817
229.052138	8000.189644	10.031770	-0.047352	4.815807
229.108533	8000.231077	10.036775	-0.047363	4.815819
228.923648	8000.166213	10.041779	-0.047328	4.815801
229.012486	8000.227372	10.046784	-0.047344	4.815818
229.062145	8000.195078	10.051789	-0.047353	4.815809
229.017555	8000.189013	10.056794	-0.047345	4.815807
228.941050	8000.221912	10.061799	-0.047331	4.815817
228.868811	8000.188730	10.066803	-0.047317	4.815808
229.128880	8000.235565	10.071808	-0.047365	4.815820
229.222849	8000.215718	10.076813	-0.047383	4.815814
228.986592	8000.209779	10.081818	-0.047338	4.815813
229.103742	8000.243652	10.086823	-0.047360	4.815823
228.942059	8000.181294	10.091827	-0.047330	4.815805
229.160399	8000.181580	10.096832	-0.047370	4.815804
229.048518	8000.209645	10.101837	-0.047349	4.815813
229.017221	8000.200592	10.106842	-0.047343	4.815811
229.191472	8000.215109	10.111847	-0.047375	4.815814
229.184793	8000.216053	10.116851	-0.047374	4.815814
229.103011	8000.229663	10.121856	-0.047359	4.815819
229.181704	8000.233044	10.126861	-0.047373	4.815819
229.126178	8000.230004	10.131866	-0.047363	4.815819
229.116479	8000.247972	10.136871	-0.047361	4.815824
229.020513	8000.212275	10.141875	-0.047343	4.815814
229.082017	8000.186572	10.146880	-0.047354	4.815806
229.110442	8000.210486	10.151885	-0.047359	4.815813
229.003009	8000.187408	10.156890	-0.047339	4.815807
229.113898	8000.213712	10.161895	-0.047359	4.815814
229.034197	8000.186811	10.166899	-0.047344	4.815807
229.133967	8000.216137	10.171904	-0.047363	4.815815
229.068816	8000.208675	10.176909	-0.047350	4.815813
228.997853	8000.155242	10.181914	-0.047337	4.815798
229.217878	8000.205702	10.186919	-0.047378	4.815811
229.213867	8000.185350	10.191923	-0.047377	4.815805
229.366293	8000.222990	10.196928	-0.047405	4.815816
229.491118	8000.212174	10.201933	-0.047428	4.815812
229.316011	8000.190144	10.206938	-0.047395	4.815806
229.351274	8000.229105	10.211943	-0.047402	4.815818
229.386812	8000.189116	10.216947	-0.047408	4.815806
229.209629	8000.213998	10.221952	-0.047375	4.815814
229.188493	8000.198707	10.226957	-0.047371	4.815809
229.113129	8000.212420	10.231962	-0.047357	4.815814
229.280075	8000.225752	10.236967	-0.047388	4.815817
229.191396	8000.189105	10.241971	-0.047371	4.815807
229.074297	8000.233090	10.246976	-0.047349	4.815820
229.218583	8000.208716	10.251981	-0.047376	4.815812
229.257220	8000.174111	10.256986	-0.047383	4.815802
229.216287	8000.231055	10.261991	-0.047375	4.815819
229.363765	8000.215268	10.266995	-0.047402	4.815813
229.313199	8000.240048	10.272000	-0.047392	4.815821
229.269380	8000.208388	10.277005	-0.047384	4.815812
229.192613	8000.196472	10.282010	-0.047370	4.815809
229.440616	8000.232444	10.287015	-0.047416	4.815818
229.420924	8000.201171	10.292019	-0.047412	4.815809
229.494782	8000.246086	10.297024	-0.047425	4.815822
229.359222	8000.250298	10.302029	-0.047400	4.815824
229.556163	8000.241706	10.307034	-0.047436	4.815820
229.362996	8000.244993	10.312039	-0.047400	4.815822
229.488139	8000.225647	10.317043	-0.047423	4.815816
229.397432	8000.229511	10.322048	-0.047406	4.815818
229.367778	8000.222618	10.327053	-0.047401	4.815816
229.134709	8000.196458	10.332058	-0.047357	4.815809
229.425566	8000.226716	10.337063	-0.047411	4.815817
229.405848	8000.202911	10.342067	-0.047407	4.815810
229.274236	8000.201851	10.347072	-0.047383	4.815810
229.325774	8000.201596	10.352077	-0.047392	4.815810
229.441976	8000.191709	10.357082	-0.047413	4.815806
229.440039	8000.245010	10.362087	-0.047413	4.815822
229.555011	8000.212697	10.367091	-0.047434	4.815812
229.533904	8000.226214	10.372096	-0.047430	4.815816
229.598754	8000.240043	10.377101	-0.047442	4.815820
229.495565	8000.217033	10.382106	-0.047423	4.815813
229.481098	8000.219986	10.387111	-0.047420	4.815814
229.527988	8000.192982	10.392115	-0.047428	4.815806
229.426322	8000.221211	10.397120	-0.047409	4.815815
229.138135	8000.194166	10.402125	-0.047355	4.815808
229.191503	8000.187538	10.407130	-0.047365	4.815806
229.409473	8000.218761	10.412135	-0.047405	4.815814
229.170225	8000.161560	10.417139	-0.047361	4.815799
229.328849	8000.202499	10.422144	-0.047390	4.815810
229.540894	8000.197351	10.427149	-0.047429	4.815808
229.512262	8000.183006	10.432154	-0.047424	4.815803
229.650325	8000.222549	10.437159	-0.047449	4.815814
229.380880	8000.207541	10.442163	-0.047399	4.815811
229.427058	8000.218936	10.447168	-0.047407	4.815814
229.509396	8000.221309	10.452173	-0.047423	4.815815
229.508974	8000.178609	10.457178	-0.047422	4.815802
229.691968	8000.217807	10.462183	-0.047456	4.815813
229.636289	8000.206229	10.467187	-0.047446	4.815810
229.772165	8000.189188	10.472192	-0.047471	4.815804
229.560133	8000.193240	10.477197	-0.047431	4.815806
229.441443	8000.137973	10.482202	-0.047409	4.815791
229.583742	8000.202124	10.487207	-0.047435	4.815809
229.673886	8000.189685	10.492211	-0.047452	4.815805
229.569927	8000.222144	10.497216	-0.047432	4.815815
229.572971	8000.237115	10.502221	-0.047433	4.815819
229.560996	8000.216635	10.507226	-0.047430	4.815813
229.671585	8000.238667	10.512231	-0.047451	4.815819
229.391231	8000.204278	10.517235	-0.047398	4.815810
229.375708	8000.186943	10.522240	-0.047395	4.815805
229.567096	8000.208137	10.527245	-0.047431	4.815811
229.472530	8000.191667	10.532250	-0.047413	4.815806
229.526949	8000.221332	10.537255	-0.047423	4.815815
229.526160	8000.178626	10.542259	-0.047423	4.815802
229.546273	8000.182135	10.547264	-0.047426	4.815803
229.610737	8000.208761	10.552269	-0.047438	4.815811
229.635345	8000.200605	10.557274	-0.047442	4.815808
229.565598	8000.218676	10.562279	-0.047429	4.815814
229.640324	8000.210257	10.567283	-0.047443	4.815811
229.764992	8000.236782	10.572288	-0.047466	4.815818
229.886700	8000.263261	10.577293	-0.047489	4.815825
229.584198	8000.216779	10.582298	-0.047432	4.815813
229.621934	8000.237642	10.587303	-0.047439	4.815819
229.635161	8000.225035	10.592307	-0.047441	4.815815
229.656748	8000.233902	10.597312	-0.047445	4.815818
229.524642	8000.246705	10.602317	-0.047420	4.815822
229.625586	8000.180024	10.607322	-0.047439	4.815802
229.682974	8000.237478	10.612327	-0.047449	4.815819
229.689254	8000.203421	10.617331	-0.047450	4.815809
229.611245	8000.209623	10.622336	-0.047436	4.815811
229.809264	8000.237326	10.627341	-0.047472	4.815818
229.593508	8000.205040	10.632346	-0.047432	4.815810
229.491180	8000.227923	10.637351	-0.047413	4.815817
229.485642	8000.209681	10.642355	-0.047412	4.815812
229.490175	8000.218274	10.647360	-0.047412	4.815814
229.559939	8000.220445	10.652365	-0.047425	4.815814
229.561863	8000.218327	10.657370	-0.047425	4.815814
229.720254	8000.258197	10.662375	-0.047455	4.815825
229.610255	8000.220140	10.667379	-0.047434	4.815814
229.607924	8000.221154	10.672384	-0.047433	4.815814
229.634122	8000.259970	10.677389	-0.047438	4.815826
229.401278	8000.214607	10.682394	-0.047394	4.815813
229.552000	8000.229814	10.687399	-0.047422	4.815817
229.664079	8000.208124	10.692403	-0.047443	4.815810
229.713551	8000.221706	10.697408	-0.047452	4.815814
229.556517	8000.230908	10.702413	-0.047423	4.815818
229.420571	8000.203104	10.707418	-0.047397	4.815810
229.661486	8000.228294	10.712423	-0.047442	4.815816
229.466713	8000.188877	10.717427	-0.047405	4.815806
229.530604	8000.199489	10.722432	-0.047417	4.815808
229.613623	8000.239217	10.727437	-0.047432	4.815820
229.506236	8000.203336	10.732442	-0.047412	4.815810
229.723655	8000.204675	10.737447	-0.047452	4.815809
229.751721	8000.196575	10.742451	-0.047458	4.815807
229.669392	8000.194172	10.747456	-0.047442	4.815806
229.794933	8000.211108	10.752461	-0.047465	4.815811
229.554828	8000.204039	10.757466	-0.047420	4.815810
229.719911	8000.225878	10.762471	-0.047451	4.815815
229.644188	8000.215045	10.767475	-0.047437	4.815813
229.525038	8000.216319	10.772480	-0.047414	4.815813
229.560341	8000.236076	10.777485	-0.047421	4.815819
229.461943	8000.191804	10.782490	-0.047402	4.815807
229.587707	8000.211944	10.787495	-0.047425	4.815812
229.727495	8000.200302	10.792499	-0.047451	4.815808
229.779534	8000.221394	10.797504	-0.047461	4.815814
229.695346	8000.196555	10.802509	-0.047445	4.815807
229.476127	8000.172750	10.807514	-0.047404	4.815801
229.747850	8000.205902	10.812519	-0.047454	4.815809
229.764643	8000.214692	10.817523	-0.047457	4.815812
229.716909	8000.201108	10.822528	-0.047448	4.815808
229.699942	8000.199753	10.827533	-0.047445	4.815808
229.674413	8000.197194	10.832538	-0.047440	4.815807
229.533871	8000.217330	10.837543	-0.047414	4.815814
229.756291	8000.204880	10.842547	-0.047455	4.815809
229.891479	8000.212369	10.847552	-0.047480	4.815811
229.667325	8000.229029	10.852557	-0.047438	4.815817
229.624007	8000.203778	10.857562	-0.047430	4.815809
229.703388	8000.197568	10.862567	-0.047444	4.815807
229.754387	8000.194103	10.867571	-0.047454	4.815806
229.681374	8000.224925	10.872576	-0.047440	4.815815
229.948115	8000.244128	10.877581	-0.047489	4.815820
229.754746	8000.215403	10.882586	-0.047453	4.815812
229.755869	8000.210071	10.887591	-0.047453	4.815811
229.658856	8000.204231	10.892595	-0.047435	4.815809
229.790257	8000.223396	10.897600	-0.047459	4.815814
229.760749	8000.257050	10.902605	-0.047454	4.815824
229.622236	8000.206799	10.907610	-0.047428	4.815810
229.615265	8000.253618	10.912615	-0.047426	4.815824
229.913308	8000.259452	10.917619	-0.047481	4.815824
229.585552	8000.212566	10.922624	-0.047420	4.815812
229.760480	8000.220693	10.927629	-0.047453	4.815814
229.694330	8000.199344	10.932634	-0.047440	4.815808
229.739679	8000.245935	10.937639	-0.047448	4.815821
229.729897	8000.197750	10.942643	-0.047446	4.815807
229.906292	8000.205900	10.947648	-0.047479	4.815809
229.938194	8000.217067	10.952653	-0.047485	4.815812
229.601048	8000.195637	10.957658	-0.047422	4.815807
229.799132	8000.250014	10.962663	-0.047459	4.815822
229.755982	8000.199160	10.967667	-0.047450	4.815808
229.579944	8000.196320	10.972672	-0.047417	4.815808
229.638821	8000.217521	10.977677	-0.047428	4.815813
229.630555	8000.192834	10.982682	-0.047426	4.815806
229.799675	8000.243545	10.987687	-0.047458	4.815820
229.704634	8000.235603	10.992691	-0.047440	4.815818
229.796013	8000.207179	10.997696	-0.047457	4.815810
229.863501	8000.245591	11.002701	-0.047469	4.815821
229.446957	8000.191946	11.007706	-0.047391	4.815807
229.566367	8000.208784	11.012711	-0.047413	4.815811
229.769742	8000.218434	11.017715	-0.047451	4.815813
229.800060	8000.210369	11.022720	-0.047457	4.815811
229.875107	8000.222228	11.027725	-0.047470	4.815814
229.759464	8000.202219	11.032730	-0.047449	4.815808
229.665437	8000.233770	11.037735	-0.047431	4.815818
229.666939	8000.195369	11.042739	-0.047431	4.815807
229.661869	8000.170732	11.047744	-0.047430	4.815800
229.771358	8000.215152	11.052749	-0.047450	4.815812
229.509513	8000.191730	11.057754	-0.047401	4.815807
229.778339	8000.236573	11.062759	-0.047451	4.815818
229.750744	8000.203039	11.067763	-0.047446	4.815809
229.725319	8000.207951	11.072768	-0.047441	4.815810
229.879125	8000.225341	11.077773	-0.047469	4.815815
229.838233	8000.203331	11.082778	-0.047462	4.815808
229.923119	8000.211079	11.087783	-0.047477	4.815810
229.886463	8000.206208	11.092787	-0.047470	4.815809
229.753777	8000.205131	11.097792	-0.047445	4.815809
229.868008	8000.234689	11.102797	-0.047466	4.815818
229.648565	8000.200211	11.107802	-0.047425	4.815808
229.747886	8000.238066	11.112807	-0.047444	4.815819
229.775640	8000.213956	11.117811	-0.047449	4.815812
229.717207	8000.203401	11.122816	-0.047438	4.815809
229.856224	8000.239759	11.127821	-0.047463	4.815819
229.814475	8000.223069	11.132826	-0.047455	4.815814
229.789708	8000.219456	11.137831	-0.047451	4.815813
229.776143	8000.196817	11.142835	-0.047448	4.815807
229.927674	8000.242979	11.147840	-0.047476	4.815820
229.836252	8000.234028	11.152845	-0.047459	4.815818
229.648103	8000.173378	11.157850	-0.047424	4.815801
229.932609	8000.191798	11.162855	-0.047476	4.815805
229.837434	8000.207327	11.167859	-0.047458	4.815810
229.856393	8000.195880	11.172864	-0.047462	4.815806
229.823971	8000.246558	11.177869	-0.047456	4.815821
229.784332	8000.218166	11.182874	-0.047448	4.815813
229.824002	8000.240126	11.187879	-0.047455	4.815819
229.830975	8000.217817	11.192883	-0.047456	4.815813
229.889437	8000.223008	11.197888	-0.047467	4.815814
230.280594	8000.242074	11.202893	-0.047540	4.815818
229.915923	8000.188193	11.207898	-0.047472	4.815804
230.020450	8000.198390	11.212903	-0.047491	4.815806
230.107671	8000.205110	11.217907	-0.047507	4.815808
230.041260	8000.236038	11.222912	-0.047495	4.815817
229.908087	8000.231751	11.227917	-0.047470	4.815817
229.700489	8000.188928	11.232922	-0.047431	4.815805
229.768280	8000.260419	11.237927	-0.047443	4.815826
229.871613	8000.230053	11.242931	-0.047462	4.815816
229.713785	8000.211501	11.247936	-0.047433	4.815812
229.978958	8000.237081	11.252941	-0.047482	4.815818
230.129460	8000.225610	11.257946	-0.047510	4.815814
229.845409	8000.229572	11.262951	-0.047457	4.815816
229.976566	8000.235930	11.267955	-0.047481	4.815818
229.942313	8000.203356	11.272960	-0.047474	4.815808
229.950416	8000.239747	11.277965	-0.047476	4.815819
229.924362	8000.214774	11.282970	-0.047471	4.815812
230.085212	8000.248282	11.287975	-0.047500	4.815821
229.907860	8000.194206	11.292979	-0.047467	4.815806
229.745291	8000.175578	11.297984	-0.047437	4.815801
229.916009	8000.196441	11.302989	-0.047468	4.815806
229.953150	8000.170348	11.307994	-0.047475	4.815798
229.988034	8000.205035	11.312999	-0.047481	4.815808
229.903262	8000.219664	11.318003	-0.047465	4.815813
229.897881	8000.223830	11.323008	-0.047464	4.815814
230.036815	8000.231379	11.328013	-0.047490	4.815816
230.032812	8000.193956	11.333018	-0.047489	4.815805
230.071173	8000.223364	11.338023	-0.047496	4.815813
230.116408	8000.212339	11.343027	-0.047504	4.815810
229.857771	8000.230579	11.348032	-0.047456	4.815817
230.096055	8000.229053	11.353037	-0.047500	4.815815
229.995247	8000.222085	11.358042	-0.047481	4.815813
229.894888	8000.236464	11.363047	-0.047462	4.815818
230.022954	8000.235303	11.368051	-0.047486	4.815817
230.135601	8000.215756	11.373056	-0.047507	4.815811
230.055728	8000.215526	11.378061	-0.047492	4.815811
229.945377	8000.210539	11.383066	-0.047471	4.815810
230.059450	8000.217689	11.388071	-0.047492	4.815812
230.223361	8000.214970	11.393075	-0.047522	4.815810
229.977493	8000.200339	11.398080	-0.047476	4.815807
230.179210	8000.234503	11.403085	-0.047514	4.815816
230.015697	8000.193453	11.408090	-0.047483	4.815805
229.954544	8000.226599	11.413095	-0.047472	4.815815
229.992392	8000.193049	11.418099	-0.047479	4.815805
229.945369	8000.200815	11.423104	-0.047470	4.815808
229.976474	8000.230107	11.428109	-0.047475	4.815816
229.936240	8000.177165	11.433114	-0.047468	4.815801
230.099286	8000.196837	11.438119	-0.047498	4.815806
230.077420	8000.210342	11.443123	-0.047493	4.815810
230.064757	8000.214391	11.448128	-0.047491	4.815811
230.124622	8000.275087	11.453133	-0.047502	4.815828
229.966281	8000.208512	11.458138	-0.047472	4.815810
229.876741	8000.215596	11.463143	-0.047455	4.815812
230.302123	8000.224542	11.468147	-0.047534	4.815813
230.054489	8000.213083	11.473152	-0.047488	4.815811
230.084714	8000.216754	11.478157	-0.047494	4.815812
229.897235	8000.204128	11.483162	-0.047458	4.815809
230.059215	8000.244055	11.488167	-0.047489	4.815820
229.971236	8000.239427	11.493171	-0.047472	4.815819
229.852988	8000.200171	11.498176	-0.047450	4.815808
229.949311	8000.211304	11.503181	-0.047467	4.815811
230.046700	8000.172307	11.508186	-0.047485	4.815799
230.148851	8000.232614	11.513191	-0.047504	4.815816
230.266805	8000.246229	11.518195	-0.047526	4.815819
230.022677	8000.220956	11.523200	-0.047480	4.815813
230.012282	8000.220774	11.528205	-0.047478	4.815813
230.070379	8000.180080	11.533210	-0.047489	4.815801
230.025184	8000.219884	11.538215	-0.047480	4.815813
230.148037	8000.218639	11.543219	-0.047503	4.815812
229.876395	8000.187591	11.548224	-0.047452	4.815804
229.868335	8000.186380	11.553229	-0.047451	4.815804
229.961727	8000.181461	11.558234	-0.047468	4.815802
230.002753	8000.227984	11.563239	-0.047475	4.815815
230.081479	8000.206826	11.568243	-0.047490	4.815809
230.261729	8000.221440	11.573248	-0.047523	4.815812
230.189349	8000.236267	11.578253	-0.047510	4.815817
229.994527	8000.203251	11.583258	-0.047473	4.815808
230.105595	8000.193281	11.588263	-0.047494	4.815805
230.212734	8000.213124	11.593267	-0.047513	4.815810
229.883077	8000.192881	11.598272	-0.047452	4.815806
230.004714	8000.232161	11.603277	-0.047474	4.815817
230.204496	8000.205477	11.608282	-0.047511	4.815808
230.137631	8000.223594	11.613287	-0.047499	4.815813
230.150604	8000.223787	11.618291	-0.047501	4.815813
230.102762	8000.241143	11.623296	-0.047492	4.815819
230.102321	8000.218714	11.628301	-0.047492	4.815812
230.094650	8000.196170	11.633306	-0.047490	4.815806
230.276749	8000.214014	11.638311	-0.047524	4.815810
230.303115	8000.212288	11.643315	-0.047528	4.815809
229.944586	8000.185180	11.648320	-0.047461	4.815803
230.032036	8000.231381	11.653325	-0.047478	4.815816
230.091538	8000.231253	11.658330	-0.047489	4.815816
229.952620	8000.214071	11.663335	-0.047462	4.815812
229.973253	8000.241061	11.668339	-0.047466	4.815819
230.028885	8000.201394	11.673344	-0.047476	4.815808
230.236665	8000.232455	11.678349	-0.047515	4.815816
230.088904	8000.189524	11.683354	-0.047487	4.815804
230.079197	8000.187219	11.688359	-0.047485	4.815803
230.357914	8000.213016	11.693363	-0.047537	4.815809
230.093865	8000.190625	11.698368	-0.047488	4.815804
229.978844	8000.225040	11.703373	-0.047466	4.815815
230.241356	8000.202564	11.708378	-0.047515	4.815807
230.099310	8000.203470	11.713383	-0.047488	4.815808
229.942466	8000.195603	11.718387	-0.047459	4.815806
229.798942	8000.177280	11.723392	-0.047432	4.815802
230.120379	8000.235771	11.728397	-0.047491	4.815817
229.964527	8000.206581	11.733402	-0.047462	4.815809
229.915454	8000.171636	11.738407	-0.047453	4.815799
230.044732	8000.168360	11.743411	-0.047477	4.815798
230.033233	8000.169227	11.748416	-0.047474	4.815798
229.952032	8000.226592	11.753421	-0.047459	4.815815
229.974936	8000.181065	11.758426	-0.047463	4.815802
230.036933	8000.178844	11.763431	-0.047475	4.815801
229.994238	8000.215487	11.768435	-0.047467	4.815812
229.856450	8000.174850	11.773440	-0.047441	4.815801
230.020436	8000.195605	11.778445	-0.047471	4.815806
229.930675	8000.183479	11.783450	-0.047454	4.815803
229.893720	8000.181804	11.788455	-0.047447	4.815803
230.074225	8000.183619	11.793459	-0.047480	4.815802
230.003640	8000.171801	11.798464	-0.047467	4.815799
230.066462	8000.203736	11.803469	-0.047479	4.815808
230.095481	8000.184981	11.808474	-0.047484	4.815803
230.211508	8000.202832	11.813479	-0.047505	4.815807
230.142645	8000.215582	11.818483	-0.047492	4.815811
230.065657	8000.199394	11.823488	-0.047478	4.815807
230.223206	8000.195506	11.828493	-0.047507	4.815805
230.156824	8000.195492	11.833498	-0.047494	4.815805
230.116287	8000.214032	11.838503	-0.047487	4.815811
230.337008	8000.230362	11.843507	-0.047528	4.815815
230.167036	8000.193476	11.848512	-0.047496	4.815805
230.102380	8000.216964	11.853517	-0.047484	4.815812
229.946692	8000.178174	11.858522	-0.047454	4.815801
230.114784	8000.201128	11.863527	-0.047486	4.815807
230.054712	8000.232158	11.868531	-0.047474	4.815817
230.020795	8000.200656	11.873536	-0.047468	4.815808
230.189190	8000.219348	11.878541	-0.047499	4.815812
230.039722	8000.184925	11.883546	-0.047471	4.815803
230.143938	8000.208988	11.888551	-0.047490	4.815809
230.318650	8000.219246	11.893555	-0.047523	4.815812
230.207599	8000.189707	11.898560	-0.047502	4.815803
230.031426	8000.225276	11.903565	-0.047469	4.815815
230.058432	8000.190484	11.908570	-0.047474	4.815804
230.311936	8000.204140	11.913575	-0.047521	4.815807
230.414131	8000.229238	11.918579	-0.047539	4.815814
230.144507	8000.198221	11.923584	-0.047489	4.815806
230.241975	8000.233913	11.928589	-0.047507	4.815816
230.233147	8000.190011	11.933594	-0.047505	4.815803
230.022934	8000.198359	11.938599	-0.047466	4.815807
230.184790	8000.236151	11.943603	-0.047496	4.815817
230.008228	8000.188490	11.948608	-0.047463	4.815804
230.162506	8000.243232	11.953613	-0.047491	4.815819
230.159513	8000.223963	11.958618	-0.047491	4.815814
230.345179	8000.233329	11.963623	-0.047525	4.815816
230.162322	8000.239982	11.968627	-0.047491	4.815818
230.175489	8000.222040	11.973632	-0.047493	4.815813
230.183199	8000.243488	11.978637	-0.047494	4.815819
230.093101	8000.200415	11.983642	-0.047477	4.815807
230.212893	8000.227929	11.988647	-0.047499	4.815815
230.227568	8000.213212	11.993651	-0.047502	4.815810
230.154618	8000.203490	11.998656	-0.047488	4.815808
230.252019	8000.243449	12.003661	-0.047506	4.815819
230.090614	8000.221638	12.008666	-0.047476	4.815813
230.268387	8000.233012	12.013671	-0.047509	4.815816
230.234818	8000.221788	12.018675	-0.047502	4.815813
230.139680	8000.204242	12.023680	-0.047485	4.815808
230.332583	8000.233996	12.028685	-0.047520	4.815816
230.151395	8000.212935	12.033690	-0.047486	4.815811
230.312399	8000.225106	12.038695	-0.047516	4.815813
230.326400	8000.238119	12.043699	-0.047519	4.815817
230.273550	8000.196711	12.048704	-0.047509	4.815805
230.267549	8000.251015	12.053709	-0.047507	4.815821
230.322211	8000.218801	12.058714	-0.047517	4.815812
230.366732	8000.209898	12.063719	-0.047525	4.815809
230.181832	8000.216518	12.068723	-0.047491	4.815812
230.088624	8000.156324	12.073728	-0.047473	4.815794
230.174824	8000.215308	12.078733	-0.047489	4.815811
230.216912	8000.197830	12.083738	-0.047497	4.815806
230.226033	8000.212898	12.088743	-0.047498	4.815810
230.422942	8000.258722	12.093747	-0.047535	4.815823
230.368450	8000.297310	12.098752	-0.047525	4.815834
230.159860	8000.275809	12.103757	-0.047486	4.815829
230.158685	8000.201087	12.108762	-0.047485	4.815807
230.159356	8000.197882	12.113767	-0.047485	4.815806
230.292329	8000.224541	12.118771	-0.047510	4.815813
230.011275	8000.195475	12.123776	-0.047457	4.815806
230.228968	8000.230962	12.128781	-0.047498	4.815816
230.253242	8000.190792	12.133786	-0.047502	4.815804
230.157471	8000.189240	12.138791	-0.047484	4.815804
230.190645	8000.211096	12.143795	-0.047490	4.815810
230.086857	8000.187009	12.148800	-0.047470	4.815803
230.037702	8000.227817	12.153805	-0.047461	4.815816
229.949681	8000.212519	12.158810	-0.047444	4.815812
229.937430	8000.226177	12.163815	-0.047442	4.815816
230.036713	8000.207483	12.168819	-0.047460	4.815810
229.823427	8000.202978	12.173824	-0.047420	4.815809
229.950280	8000.211400	12.178829	-0.047444	4.815811
230.134097	8000.195130	12.183834	-0.047478	4.815806
229.962374	8000.201961	12.188839	-0.047446	4.815808
229.893567	8000.221114	12.193843	-0.047433	4.815814
230.005601	8000.197290	12.198848	-0.047453	4.815807
230.106213	8000.225563	12.203853	-0.047472	4.815815
230.192225	8000.173580	12.208858	-0.047488	4.815799
230.079179	8000.204827	12.213863	-0.047467	4.815809
230.307943	8000.228755	12.218867	-0.047509	4.815815
230.166552	8000.207265	12.223872	-0.047483	4.815809
230.259162	8000.223674	12.228877	-0.047500	4.815813
230.228921	8000.212504	12.233882	-0.047494	4.815810
230.153520	8000.192073	12.238887	-0.047480	4.815805
230.196633	8000.188482	12.243891	-0.047487	4.815803
229.924307	8000.218239	12.248896	-0.047437	4.815813
230.063836	8000.220463	12.253901	-0.047462	4.815813
230.122103	8000.221383	12.258906	-0.047473	4.815813
230.156560	8000.213385	12.263911	-0.047479	4.815811
230.322439	8000.224568	12.268915	-0.047510	4.815813
230.002532	8000.203414	12.273920	-0.047450	4.815809
229.930731	8000.217184	12.278925	-0.047437	4.815813
230.043468	8000.194438	12.283930	-0.047457	4.815806
230.204396	8000.213010	12.288935	-0.047487	4.815811
230.165424	8000.256115	12.293939	-0.047480	4.815823
230.042348	8000.203977	12.298944	-0.047457	4.815809
230.107493	8000.193271	12.303949	-0.047469	4.815805
230.267434	8000.217161	12.308954	-0.047498	4.815812
230.320760	8000.199864	12.313959	-0.047508	4.815806
230.309961	8000.217813	12.318963	-0.047506	4.815812
230.095854	8000.178086	12.323968	-0.047466	4.815801
229.970706	8000.231544	12.328973	-0.047442	4.815817
230.219326	8000.188572	12.333978	-0.047488	4.815803
230.323220	8000.222233	12.338983	-0.047508	4.815813
230.304251	8000.246454	12.343987	-0.047504	4.815820
230.103165	8000.206935	12.348992	-0.047466	4.815809
230.106549	8000.214443	12.353997	-0.047467	4.815812
230.001953	8000.189276	12.359002	-0.047447	4.815805
230.185549	8000.191140	12.364007	-0.047481	4.815804
230.266098	8000.232962	12.369011	-0.047496	4.815816
230.066060	8000.215866	12.374016	-0.047459	4.815812
229.942618	8000.223473	12.379021	-0.047435	4.815815
230.229699	8000.239801	12.384026	-0.047489	4.815818
230.334513	8000.242535	12.389031	-0.047508	4.815819
230.305499	8000.239920	12.394035	-0.047502	4.815818
230.143012	8000.212757	12.399040	-0.047472	4.815811
230.122950	8000.219889	12.404045	-0.047468	4.815813
230.086848	8000.199022	12.409050	-0.047461	4.815807
230.124992	8000.200686	12.414055	-0.047468	4.815808
230.150872	8000.210688	12.419059	-0.047473	4.815810
229.956155	8000.162736	12.424064	-0.047436	4.815797
230.053537	8000.222966	12.429069	-0.047454	4.815814
229.912303	8000.208948	12.434074	-0.047428	4.815811
230.208235	8000.211548	12.439079	-0.047483	4.815810
230.273605	8000.218984	12.444083	-0.047495	4.815812
230.116234	8000.212175	12.449088	-0.047465	4.815811
230.069784	8000.221017	12.454093	-0.047456	4.815814
229.917873	8000.203627	12.459098	-0.047428	4.815809
229.875521	8000.209334	12.464103	-0.047420	4.815811
230.127764	8000.209098	12.469107	-0.047467	4.815810
230.080502	8000.188053	12.474112	-0.047458	4.815804
230.053977	8000.192947	12.479117	-0.047453	4.815806
230.257973	8000.204741	12.484122	-0.047490	4.815808
230.161712	8000.178641	12.489127	-0.047472	4.815801
230.234301	8000.234205	12.494131	-0.047486	4.815817
229.834298	8000.177624	12.499136	-0.047411	4.815802
230.210639	8000.223125	12.504141	-0.047481	4.815814
230.303954	8000.210737	12.509146	-0.047498	4.815810
230.135584	8000.225091	12.514151	-0.047467	4.815815
230.190198	8000.221685	12.519155	-0.047477	4.815813
230.089906	8000.209391	12.524160	-0.047458	4.815810
229.998540	8000.229248	12.529165	-0.047440	4.815817
230.043487	8000.210749	12.534170	-0.047449	4.815811
230.112221	8000.200100	12.539175	-0.047461	4.815808
230.293093	8000.246733	12.544179	-0.047495	4.815820
230.010396	8000.222976	12.549184	-0.047442	4.815815
230.298798	8000.236125	12.554189	-0.047496	4.815817
230.302204	8000.214825	12.559194	-0.047496	4.815811
230.168044	8000.193451	12.564199	-0.047471	4.815805
230.253877	8000.230023	12.569203	-0.047487	4.815816
229.921073	8000.195860	12.574208	-0.047424	4.815807
229.957128	8000.232700	12.579213	-0.047431	4.815818
229.894036	8000.198596	12.584218	-0.047419	4.815808
230.033269	8000.202949	12.589223	-0.047445	4.815809
230.056851	8000.210781	12.594227	-0.047449	4.815811
230.083318	8000.187718	12.599232	-0.047454	4.815804
230.142596	8000.221729	12.604237	-0.047465	4.815814
230.171215	8000.205102	12.609242	-0.047470	4.815809
230.094859	8000.202795	12.614247	-0.047455	4.815808
230.084838	8000.207953	12.619251	-0.047453	4.815810
229.933073	8000.171360	12.624256	-0.047425	4.815800
230.096876	8000.207049	12.629261	-0.047455	4.815810
230.302054	8000.195389	12.634266	-0.047493	4.815805
230.379706	8000.211557	12.639271	-0.047508	4.815810
230.548546	8000.222788	12.644275	-0.047539	4.815812
230.301952	8000.168668	12.649280	-0.047493	4.815798
230.358411	8000.199433	12.654285	-0.047503	4.815806
230.311598	8000.207203	12.659290	-0.047494	4.815809
230.416514	8000.181130	12.664295	-0.047514	4.815801
230.364477	8000.214423	12.669299	-0.047504	4.815811
230.221432	8000.186505	12.674304	-0.047477	4.815803
230.123138	8000.209452	12.679309	-0.047458	4.815810
230.214372	8000.185294	12.684314	-0.047475	4.815803
230.232939	8000.181309	12.689319	-0.047478	4.815802
230.238292	8000.210188	12.694323	-0.047479	4.815810
230.255103	8000.206174	12.699328	-0.047482	4.815809
230.381849	8000.230599	12.704333	-0.047506	4.815815
230.428558	8000.202526	12.709338	-0.047514	4.815807
230.180654	8000.155854	12.714343	-0.047468	4.815794
230.402120	8000.221277	12.719347	-0.047509	4.815813
230.306039	8000.196246	12.724352	-0.047491	4.815806
230.319542	8000.224189	12.729357	-0.047493	4.815814
230.243658	8000.199483	12.734362	-0.047479	4.815807
230.194245	8000.194407	12.739367	-0.047469	4.815806
230.360723	8000.229072	12.744371	-0.047500	4.815815
230.227378	8000.191707	12.749376	-0.047475	4.815805
230.283856	8000.224607	12.754381	-0.047486	4.815814
230.251653	8000.227276	12.759386	-0.047480	4.815815
230.351580	8000.211793	12.764391	-0.047498	4.815810
230.404698	8000.246773	12.769395	-0.047508	4.815820
230.362046	8000.188457	12.774400	-0.047500	4.815803
230.406986	8000.224373	12.779405	-0.047508	4.815813
230.390659	8000.189953	12.784410	-0.047504	4.815803
230.435277	8000.183185	12.789415	-0.047513	4.815801
230.436468	8000.218399	12.794419	-0.047513	4.815812
230.218496	8000.190345	12.799424	-0.047472	4.815804
230.353501	8000.212769	12.804429	-0.047497	4.815810
230.456994	8000.226151	12.809434	-0.047516	4.815814
230.361560	8000.188328	12.814439	-0.047498	4.815803
230.372709	8000.207697	12.819443	-0.047500	4.815809
230.265502	8000.187823	12.824448	-0.047480	4.815803
230.274896	8000.199695	12.829453	-0.047481	4.815807
230.559945	8000.212790	12.834458	-0.047534	4.815809
230.308041	8000.186326	12.839463	-0.047487	4.815803
230.335200	8000.212354	12.844467	-0.047492	4.815810
230.139604	8000.183593	12.849472	-0.047455	4.815803
230.093237	8000.191369	12.854477	-0.047447	4.815805
230.234233	8000.201085	12.859482	-0.047473	4.815808
230.348336	8000.199700	12.864487	-0.047494	4.815807
230.333570	8000.220787	12.869491	-0.047491	4.815813
230.482279	8000.190082	12.874496	-0.047518	4.815803
230.255947	8000.177899	12.879501	-0.047476	4.815801
230.412085	8000.210265	12.884506	-0.047505	4.815809
230.295270	8000.165697	12.889511	-0.047483	4.815797
230.348694	8000.217753	12.894515	-0.047493	4.815812
230.101000	8000.156147	12.899520	-0.047446	4.815795
230.177095	8000.190429	12.904525	-0.047460	4.815805
230.395421	8000.209921	12.909530	-0.047501	4.815809
230.291690	8000.192237	12.914535	-0.047481	4.815805
230.454014	8000.201229	12.919539	-0.047512	4.815807
230.368778	8000.176372	12.924544	-0.047495	4.815800
230.307396	8000.192443	12.929549	-0.047484	4.815805
230.220543	8000.172896	12.934554	-0.047467	4.815799
230.360802	8000.183667	12.939559	-0.047493	4.815802
230.383310	8000.221357	12.944563	-0.047497	4.815813
230.408164	8000.210004	12.949568	-0.047502	4.815809
230.228810	8000.203910	12.954573	-0.047468	4.815808
230.297196	8000.180452	12.959578	-0.047481	4.815801
230.276999	8000.196117	12.964583	-0.047477	4.815806
230.184496	8000.219157	12.969587	-0.047460	4.815813
230.284826	8000.178074	12.974592	-0.047478	4.815801
230.219264	8000.190877	12.979597	-0.047466	4.815805
230.227989	8000.184600	12.984602	-0.047467	4.815803
230.161899	8000.190993	12.989607	-0.047455	4.815805
230.274648	8000.232265	12.994611	-0.047475	4.815817
230.240409	8000.217830	12.999616	-0.047469	4.815813
230.166258	8000.192084	13.004621	-0.047455	4.815805
230.204581	8000.202287	13.009626	-0.047462	4.815808
230.139805	8000.185228	13.014631	-0.047450	4.815803
230.239369	8000.198547	13.019635	-0.047468	4.815807
230.135563	8000.179795	13.024640	-0.047449	4.815802
230.444227	8000.205005	13.029645	-0.047506	4.815808
230.371479	8000.234764	13.034650	-0.047492	4.815817
230.388051	8000.209408	13.039655	-0.047495	4.815809
230.266828	8000.211715	13.044659	-0.047472	4.815811
230.291862	8000.171557	13.049664	-0.047477	4.815799
230.179362	8000.196410	13.054669	-0.047456	4.815807
230.310104	8000.201694	13.059674	-0.047480	4.815808
230.354116	8000.210921	13.064679	-0.047488	4.815810
230.453250	8000.234903	13.069683	-0.047506	4.815817
230.216652	8000.184144	13.074688	-0.047462	4.815803
230.139043	8000.180750	13.079693	-0.047447	4.815802
230.078795	8000.194705	13.084698	-0.047436	4.815807
229.939207	8000.166844	13.089703	-0.047410	4.815799
230.219897	8000.227881	13.094707	-0.047462	4.815816
230.305857	8000.168429	13.099712	-0.047478	4.815798
230.131574	8000.202960	13.104717	-0.047445	4.815809
230.234873	8000.189665	13.109722	-0.047464	4.815804
230.149491	8000.169075	13.114727	-0.047448	4.815799
230.121544	8000.228361	13.119731	-0.047443	4.815816
230.115504	8000.188771	13.124736	-0.047441	4.815805
230.150613	8000.204257	13.129741	-0.047448	4.815809
230.202345	8000.215741	13.134746	-0.047457	4.815812
229.994160	8000.205984	13.139751	-0.047418	4.815810
230.266118	8000.209265	13.144755	-0.047469	4.815810
230.254944	8000.199468	13.149760	-0.047466	4.815807
230.366203	8000.209774	13.154765	-0.047487	4.815810
230.395705	8000.195295	13.159770	-0.047492	4.815805
230.196183	8000.172873	13.164775	-0.047455	4.815800
230.371135	8000.226879	13.169779	-0.047487	4.815815
230.248624	8000.200358	13.174784	-0.047464	4.815808
230.226975	8000.211732	13.179789	-0.047460	4.815811
230.433673	8000.222502	13.184794	-0.047498	4.815813
230.316091	8000.187524	13.189799	-0.047476	4.815803
230.176995	8000.221554	13.194803	-0.047450	4.815814
230.310981	8000.213019	13.199808	-0.047475	4.815811
230.298505	8000.156255	13.204813	-0.047472	4.815794
230.347161	8000.170891	13.209818	-0.047481	4.815798
230.159428	8000.156127	13.214823	-0.047446	4.815795
230.329607	8000.196186	13.219827	-0.047478	4.815806
230.195813	8000.189756	13.224832	-0.047453	4.815805
230.302327	8000.186115	13.229837	-0.047472	4.815803
230.457882	8000.235542	13.234842	-0.047501	4.815817
230.301483	8000.175401	13.239847	-0.047472	4.815800
230.371228	8000.212782	13.244851	-0.047485	4.815811
230.453416	8000.205550	13.249856	-0.047500	4.815808
230.381226	8000.218247	13.254861	-0.047486	4.815812
230.335741	8000.198296	13.259866	-0.047477	4.815807
230.169916	8000.174281	13.264871	-0.047446	4.815800
230.464074	8000.144843	13.269875	-0.047501	4.815790
230.466421	8000.126727	13.274880	-0.047501	4.815785
230.489023	8000.182557	13.279885	-0.047505	4.815801
230.589283	8000.206557	13.284890	-0.047524	4.815808
230.375922	8000.186046	13.289895	-0.047484	4.815803
230.473177	8000.200395	13.294899	-0.047502	4.815807
230.517432	8000.192555	13.299904	-0.047510	4.815804
230.489058	8000.194218	13.304909	-0.047504	4.815805
230.420345	8000.224042	13.309914	-0.047491	4.815814
230.547056	8000.175913	13.314919	-0.047515	4.815799
230.635509	8000.212527	13.319923	-0.047531	4.815809
230.484417	8000.193016	13.324928	-0.047503	4.815804
230.415891	8000.199370	13.329933	-0.047490	4.815807
230.411559	8000.218490	13.334938	-0.047489	4.815812
230.415643	8000.205737	13.339943	-0.047490	4.815808
230.318588	8000.211633	13.344947	-0.047471	4.815811
230.317743	8000.199868	13.349952	-0.047471	4.815807
230.385673	8000.216947	13.354957	-0.047483	4.815812
230.336513	8000.236415	13.359962	-0.047474	4.815818
230.332790	8000.201130	13.364967	-0.047473	4.815808
230.346268	8000.236541	13.369971	-0.047476	4.815818
230.229603	8000.209047	13.374976	-0.047454	4.815810
230.419101	8000.231278	13.379981	-0.047489	4.815816
230.592353	8000.269253	13.384986	-0.047521	4.815826
230.455270	8000.222225	13.389991	-0.047495	4.815813
230.422367	8000.245155	13.394995	-0.047489	4.815820
230.493351	8000.228141	13.400000	-0.047502	4.815815
230.382988	8000.226354	13.405005	-0.047481	4.815815
230.602328	8000.247998	13.410010	-0.047522	4.815820
230.598706	8000.198844	13.415015	-0.047521	4.815806
230.647564	8000.223086	13.420019	-0.047530	4.815813
230.623116	8000.218411	13.425024	-0.047525	4.815811
230.586093	8000.221002	13.430029	-0.047518	4.815812
230.529876	8000.221152	13.435034	-0.047507	4.815813
230.427836	8000.221633	13.440039	-0.047488	4.815813
230.459285	8000.264801	13.445043	-0.047494	4.815826
230.337115	8000.215879	13.450048	-0.047471	4.815812
230.317883	8000.225157	13.455053	-0.047467	4.815815
230.294199	8000.226896	13.460058	-0.047463	4.815815
230.262588	8000.225307	13.465063	-0.047457	4.815815
230.513480	8000.236787	13.470067	-0.047503	4.815817
230.654715	8000.223034	13.475072	-0.047529	4.815813
230.334793	8000.221085	13.480077	-0.047470	4.815813
230.410091	8000.228680	13.485082	-0.047483	4.815815
230.366148	8000.194884	13.490087	-0.047475	4.815806
230.386149	8000.207993	13.495091	-0.047479	4.815809
230.604515	8000.185875	13.500096	-0.047519	4.815802
230.452279	8000.194086	13.505101	-0.047491	4.815805
230.396548	8000.234788	13.510106	-0.047480	4.815817
230.260606	8000.205918	13.515111	-0.047455	4.815809
230.484343	8000.228698	13.520115	-0.047496	4.815815
230.283216	8000.208384	13.525120	-0.047458	4.815810
230.159665	8000.217056	13.530125	-0.047435	4.815813
230.376486	8000.232256	13.535130	-0.047475	4.815817
230.477397	8000.197584	13.540135	-0.047494	4.815806
230.412786	8000.238143	13.545139	-0.047482	4.815818
230.283401	8000.214712	13.550144	-0.047458	4.815812
230.491741	8000.220175	13.555149	-0.047496	4.815813
230.608012	8000.243365	13.560154	-0.047518	4.815819
230.424088	8000.195585	13.565159	-0.047483	4.815806
230.575185	8000.238540	13.570163	-0.047511	4.815818
230.537010	8000.203769	13.575168	-0.047504	4.815808
230.517378	8000.207706	13.580173	-0.047500	4.815809
230.524041	8000.236606	13.585178	-0.047501	4.815817
230.500850	8000.217013	13.590183	-0.047497	4.815812
230.521988	8000.241878	13.595187	-0.047500	4.815819
230.444544	8000.251289	13.600192	-0.047486	4.815822
230.503828	8000.208480	13.605197	-0.047497	4.815809
230.554613	8000.221016	13.610202	-0.047506	4.815813
230.467674	8000.218539	13.615207	-0.047490	4.815812
230.621275	8000.227391	13.620211	-0.047518	4.815814
230.645609	8000.237369	13.625216	-0.047522	4.815817
230.521328	8000.207618	13.630221	-0.047499	4.815809
230.605010	8000.222816	13.635226	-0.047514	4.815813
230.558103	8000.175102	13.640231	-0.047505	4.815799
230.675826	8000.239927	13.645235	-0.047527	4.815818
230.658746	8000.203360	13.650240	-0.047524	4.815807
230.647988	8000.231981	13.655245	-0.047522	4.815815
230.692759	8000.263626	13.660250	-0.047530	4.815824
230.592501	8000.226792	13.665255	-0.047511	4.815814
230.809427	8000.234526	13.670259	-0.047551	4.815815
230.590501	8000.217127	13.675264	-0.047510	4.815811
230.483139	8000.218589	13.680269	-0.047490	4.815812
230.611393	8000.223833	13.685274	-0.047514	4.815813
230.553210	8000.186608	13.690279	-0.047503	4.815803
230.719539	8000.241543	13.695283	-0.047534	4.815818
230.511021	8000.207239	13.700288	-0.047495	4.815809
230.616041	8000.211043	13.705293	-0.047514	4.815809
230.579340	8000.211506	13.710298	-0.047507	4.815810
230.633329	8000.192085	13.715303	-0.047517	4.815804
230.741680	8000.239688	13.720307	-0.047537	4.815817
230.668510	8000.210758	13.725312	-0.047523	4.815809
230.460474	8000.225542	13.730317	-0.047484	4.815814
230.466358	8000.237358	13.735322	-0.047485	4.815818
230.575330	8000.212418	13.740327	-0.047505	4.815810
230.590997	8000.251065	13.745331	-0.047508	4.815821
230.543267	8000.214006	13.750336	-0.047499	4.815811
230.459390	8000.220114	13.755341	-0.047483	4.815813
230.705005	8000.219773	13.760346	-0.047529	4.815812
230.500899	8000.197276	13.765351	-0.047490	4.815806
230.367027	8000.243126	13.770355	-0.047465	4.815820
230.569128	8000.204743	13.775360	-0.047503	4.815808
230.492189	8000.182154	13.780365	-0.047488	4.815802
230.443311	8000.203760	13.785370	-0.047479	4.815808
230.471679	8000.183928	13.790375	-0.047484	4.815802
230.502252	8000.207877	13.795379	-0.047490	4.815809
230.627433	8000.215205	13.800384	-0.047513	4.815811
230.664682	8000.225390	13.805389	-0.047520	4.815813
230.655776	8000.256174	13.810394	-0.047518	4.815823
230.512813	8000.204784	13.815399	-0.047491	4.815808
230.614847	8000.216009	13.820403	-0.047510	4.815811
230.711847	8000.198345	13.825408	-0.047528	4.815805
230.784170	8000.195223	13.830413	-0.047541	4.815804
230.777824	8000.220713	13.835418	-0.047540	4.815812
230.622856	8000.208608	13.840423	-0.047510	4.815809
230.722487	8000.232598	13.845427	-0.047529	4.815815
230.698226	8000.204453	13.850432	-0.047524	4.815807
230.632589	8000.201250	13.855437	-0.047512	4.815807
230.692532	8000.209666	13.860442	-0.047523	4.815809
230.571032	8000.208767	13.865447	-0.047500	4.815809
230.655353	8000.220775	13.870451	-0.047515	4.815812
230.865015	8000.223058	13.875456	-0.047554	4.815812
230.769308	8000.203368	13.880461	-0.047536	4.815807
230.682504	8000.214763	13.885466	-0.047520	4.815810
230.581920	8000.188594	13.890471	-0.047501	4.815803
230.714765	8000.206715	13.895475	-0.047526	4.815808
230.747348	8000.217892	13.900480	-0.047532	4.815811
230.806943	8000.235905	13.905485	-0.047542	4.815816
230.846303	8000.241857	13.910490	-0.047550	4.815818
230.745678	8000.197548	13.915495	-0.047531	4.815805
230.612943	8000.247683	13.920499	-0.047506	4.815820
230.808975	8000.214538	13.925504	-0.047542	4.815810
230.797588	8000.220741	13.930509	-0.047540	4.815812
230.776564	8000.240661	13.935514	-0.047536	4.815818
230.774750	8000.206474	13.940519	-0.047535	4.815808
230.702515	8000.231974	13.945523	-0.047522	4.815815
230.770123	8000.251182	13.950528	-0.047534	4.815821
230.646534	8000.233179	13.955533	-0.047511	4.815816
230.759489	8000.260584	13.960538	-0.047532	4.815823
230.622300	8000.198616	13.965543	-0.047506	4.815806
230.435469	8000.240415	13.970547	-0.047471	4.815819
230.759244	8000.199717	13.975552	-0.047531	4.815806
230.699434	8000.200876	13.980557	-0.047520	4.815806
230.507019	8000.221246	13.985562	-0.047484	4.815813
230.411600	8000.194092	13.990567	-0.047466	4.815806
230.703909	8000.228643	13.995571	-0.047520	4.815814
230.730463	8000.225853	14.000576	-0.047525	4.815813
230.552055	8000.203769	14.005581	-0.047491	4.815808
230.498993	8000.245581	14.010586	-0.047481	4.815820
230.536332	8000.207754	14.015591	-0.047488	4.815809
230.612128	8000.215357	14.020595	-0.047502	4.815811
230.433754	8000.206078	14.025600	-0.047469	4.815809
230.665571	8000.218318	14.030605	-0.047512	4.815812
230.607430	8000.229107	14.035610	-0.047501	4.815815
230.722937	8000.208539	14.040615	-0.047522	4.815808
230.832864	8000.225226	14.045619	-0.047542	4.815813
230.561548	8000.213387	14.050624	-0.047492	4.815811
230.382643	8000.191296	14.055629	-0.047458	4.815805
230.591358	8000.224505	14.060634	-0.047497	4.815814
230.454592	8000.183884	14.065639	-0.047471	4.815803
230.360831	8000.206905	14.070643	-0.047454	4.815810
230.430254	8000.209070	14.075648	-0.047466	4.815810
230.527599	8000.212751	14.080653	-0.047484	4.815811
230.500796	8000.221908	14.085658	-0.047479	4.815813
230.412199	8000.199132	14.090663	-0.047462	4.815807
230.594123	8000.222309	14.095667	-0.047496	4.815813
230.649766	8000.224254	14.100672	-0.047506	4.815813
230.516197	8000.213559	14.105677	-0.047481	4.815811
230.682536	8000.220481	14.110682	-0.047512	4.815812
230.692862	8000.175819	14.115687	-0.047514	4.815799
230.832703	8000.231397	14.120691	-0.047540	4.815815
230.713744	8000.223070	14.125696	-0.047517	4.815813
230.680257	8000.233187	14.130701	-0.047511	4.815816
230.666894	8000.250029	14.135706	-0.047508	4.815821
230.662543	8000.207265	14.140711	-0.047507	4.815808
230.733373	8000.241463	14.145715	-0.047520	4.815818
230.577787	8000.218678	14.150720	-0.047491	4.815812
230.422549	8000.201235	14.155725	-0.047462	4.815808
230.486725	8000.220388	14.160730	-0.047474	4.815813
230.611546	8000.188233	14.165735	-0.047497	4.815803
230.424943	8000.194826	14.170739	-0.047462	4.815806
230.510750	8000.201522	14.175744	-0.047478	4.815808
230.555779	8000.196895	14.180749	-0.047486	4.815806
230.590742	8000.201708	14.185754	-0.047492	4.815807
230.556575	8000.196877	14.190759	-0.047486	4.815806
230.556737	8000.189396	14.195763	-0.047486	4.815804
230.728410	8000.214542	14.200768	-0.047517	4.815810
230.568550	8000.207693	14.205773	-0.047487	4.815809
230.594224	8000.231563	14.210778	-0.047492	4.815816
230.595920	8000.197432	14.215783	-0.047492	4.815806
230.516305	8000.213211	14.220787	-0.047477	4.815811
230.520258	8000.192987	14.225792	-0.047478	4.815805
230.310774	8000.180008	14.230797	-0.047439	4.815802
230.602511	8000.228419	14.235802	-0.047493	4.815815
230.450162	7999.265723	14.240807	-0.047464	4.815534

230.561233	7996.058565	14.245811	-0.047482	4.814595
230.584137	7990.623952	14.250816	-0.047483	4.813004
230.514402	7983.946791	14.255821	-0.047465	4.811049
230.491127	7976.623171	14.260826	-0.047456	4.808904
230.375043	7968.996843	14.265831	-0.047429	4.806669
230.389502	7961.184488	14.270835	-0.047426	4.804378
230.167273	7953.390419	14.275840	-0.047380	4.802092
230.331423	7945.339993	14.280845	-0.047405	4.799729
230.378455	7937.457585	14.285850	-0.047408	4.797414
230.237342	7929.414799	14.290855	-0.047377	4.795051
230.204017	7921.407295	14.295859	-0.047365	4.792698
230.121426	7913.380771	14.300864	-0.047344	4.790337
230.072629	7905.407505	14.305869	-0.047330	4.787991
230.035186	7897.423483	14.310874	-0.047317	4.785641
230.089087	7889.435091	14.315879	-0.047322	4.783288
229.980967	7881.442128	14.320883	-0.047297	4.780933
230.017396	7873.460324	14.325888	-0.047298	4.778580
230.094571	7865.401490	14.330893	-0.047307	4.776202
230.141078	7857.354723	14.335898	-0.047310	4.773828
229.939952	7849.399792	14.340903	-0.047267	4.771479
230.028549	7841.363646	14.345907	-0.047278	4.769105
229.926404	7833.392549	14.350912	-0.047254	4.766750
229.784459	7825.362694	14.355917	-0.047222	4.764376
229.973186	7817.424092	14.360922	-0.047252	4.762026
229.760506	7809.386691	14.365927	-0.047207	4.759648
229.828781	7801.408198	14.370931	-0.047214	4.757285
229.873420	7793.378613	14.375936	-0.047217	4.754906
229.665578	7785.343983	14.380941	-0.047173	4.752525
229.908631	7777.347739	14.385946	-0.047213	4.750152
229.902452	7769.346487	14.390951	-0.047206	4.747778
229.765987	7761.315320	14.395955	-0.047176	4.745394
229.778652	7753.379069	14.400960	-0.047173	4.743036
229.484370	7745.317705	14.405965	-0.047112	4.740642
229.530502	7737.370905	14.410970	-0.047116	4.738279
229.500759	7729.380126	14.415975	-0.047105	4.735901
229.546438	7721.308092	14.420979	-0.047108	4.733499
229.515901	7713.342169	14.425984	-0.047097	4.731127
229.592200	7705.346644	14.430989	-0.047106	4.728744
229.728625	7697.290735	14.435994	-0.047126	4.726342
229.350528	7689.336003	14.440999	-0.047050	4.723971
229.326618	7681.325611	14.446003	-0.047040	4.721581
229.611799	7673.329128	14.451008	-0.047088	4.719193
229.399481	7665.368166	14.456013	-0.047043	4.716815
229.260615	7657.334592	14.461018	-0.047012	4.714415
229.361246	7649.325772	14.466023	-0.047025	4.712020
229.361298	7641.280606	14.471027	-0.047019	4.709613
229.306663	7633.343450	14.476032	-0.047004	4.707238
229.160554	7625.246055	14.481037	-0.046971	4.704813
229.340029	7617.383249	14.486042	-0.046999	4.702457
229.188130	7609.323267	14.491047	-0.046966	4.700041
229.214408	7601.337321	14.496051	-0.046965	4.697646
229.353214	7593.312459	14.501056	-0.046986	4.695238
229.249633	7585.302689	14.506061	-0.046961	4.692833
229.032637	7577.255888	14.511066	-0.046915	4.690416
229.065912	7569.314435	14.516071	-0.046916	4.688030
229.184963	7561.297561	14.521075	-0.046933	4.685619
229.210528	7553.313336	14.526080	-0.046932	4.683217
228.865496	7545.298155	14.531085	-0.046862	4.680805
228.953771	7537.309041	14.536090	-0.046874	4.678399
228.749247	7529.314361	14.541095	-0.046830	4.675990
228.730212	7521.228431	14.546099	-0.046821	4.673552
228.847123	7513.193882	14.551104	-0.046837	4.671129
228.813133	7505.174228	14.556109	-0.046826	4.668708
228.820247	7497.214734	14.561114	-0.046822	4.666305
228.628682	7489.252415	14.566119	-0.046781	4.663900
228.536633	7481.293602	14.571123	-0.046758	4.661494
228.797241	7473.259601	14.576128	-0.046801	4.659065
228.612688	7465.225222	14.581133	-0.046761	4.656634
228.737300	7457.266128	14.586138	-0.046779	4.654224
228.726269	7449.250980	14.591143	-0.046772	4.651797
228.310013	7441.195748	14.596147	-0.046689	4.649356
228.725255	7433.240530	14.601152	-0.046761	4.646943
228.532172	7425.218028	14.606157	-0.046719	4.644510
228.449736	7417.259672	14.611162	-0.046699	4.642094
228.474871	7409.233743	14.616167	-0.046698	4.639657
228.425540	7401.263276	14.621171	-0.046683	4.637235
228.341334	7393.211738	14.626176	-0.046662	4.634788
228.203466	7385.184954	14.631181	-0.046631	4.632346
228.311387	7377.219113	14.636186	-0.046646	4.629922
228.092451	7369.202826	14.641191	-0.046600	4.627481
227.970586	7361.162233	14.646195	-0.046572	4.625032
228.064138	7353.244823	14.651200	-0.046584	4.622618
227.935614	7345.183076	14.656205	-0.046554	4.620160
227.909011	7337.208533	14.661210	-0.046544	4.617726
227.932779	7329.206511	14.666215	-0.046543	4.615283
227.979117	7321.155583	14.671219	-0.046546	4.612824
228.016130	7313.164093	14.676224	-0.046548	4.610382
227.871261	7305.184116	14.681229	-0.046516	4.607942
227.836082	7297.152217	14.686234	-0.046504	4.605484
228.039507	7289.213059	14.691239	-0.046536	4.603054
228.059691	7281.201839	14.696243	-0.046534	4.600601
227.940516	7273.246035	14.701248	-0.046507	4.598163
227.734422	7265.168424	14.706253	-0.046463	4.595686
227.717301	7257.112189	14.711258	-0.046454	4.593215
227.670574	7249.078673	14.716263	-0.046440	4.590749
227.906852	7241.132186	14.721267	-0.046479	4.588309
227.904279	7233.140667	14.726272	-0.046473	4.585853
227.582957	7225.140085	14.731277	-0.046408	4.583393
227.725357	7217.158826	14.736282	-0.046429	4.580939
227.831381	7209.158584	14.741287	-0.046443	4.578477
227.571975	7201.140499	14.746291	-0.046390	4.576007
227.501426	7193.124169	14.751296	-0.046371	4.573538
227.510071	7185.086601	14.756301	-0.046367	4.571060
227.467262	7177.116339	14.761306	-0.046354	4.568602
227.398308	7169.138360	14.766311	-0.046336	4.566140
227.458925	7161.162147	14.771315	-0.046342	4.563677
227.353448	7153.184901	14.776320	-0.046317	4.561213
227.259219	7145.107956	14.781325	-0.046294	4.558716
227.295200	7137.179173	14.786330	-0.046295	4.556264
227.327057	7129.163891	14.791335	-0.046296	4.553784
227.322067	7121.099734	14.796339	-0.046289	4.551287
227.256210	7113.150167	14.801344	-0.046272	4.548824
227.227782	7105.113091	14.806349	-0.046261	4.546333
227.358653	7097.139904	14.811354	-0.046280	4.543861
227.313867	7089.157984	14.816359	-0.046266	4.541384
227.227016	7081.121387	14.821363	-0.046245	4.538889
227.186947	7073.154267	14.826368	-0.046232	4.536415
227.158444	7065.101059	14.831373	-0.046221	4.533912
227.150386	7057.127458	14.836378	-0.046214	4.531432
226.932986	7049.121569	14.841383	-0.046168	4.528941
226.880523	7041.125016	14.846387	-0.046153	4.526451
226.991106	7033.139709	14.851392	-0.046168	4.523964
227.004858	7025.147471	14.856397	-0.046166	4.521474
226.808628	7017.148252	14.861402	-0.046124	4.518979
226.701717	7009.131820	14.866407	-0.046098	4.516477
226.802728	7001.104193	14.871411	-0.046112	4.513972
227.021948	6993.031046	14.876416	-0.046147	4.511451
226.783835	6985.037134	14.881421	-0.046097	4.508952
226.798196	6977.065521	14.886426	-0.046095	4.506459
226.735311	6969.075067	14.891431	-0.046078	4.503959
226.583839	6961.087893	14.896435	-0.046044	4.501458
226.479799	6953.111762	14.901440	-0.046019	4.498960
226.564913	6945.082546	14.906445	-0.046030	4.496444
226.684344	6937.054481	14.911450	-0.046047	4.493927
226.540524	6929.051379	14.916455	-0.046014	4.491416
226.682835	6921.042981	14.921459	-0.046035	4.488902
226.612277	6913.081945	14.926464	-0.046017	4.486401
226.464876	6905.061632	14.931469	-0.045984	4.483880
226.566486	6897.065084	14.936474	-0.045998	4.481366
226.523989	6889.095386	14.941479	-0.045984	4.478859
226.377313	6881.077785	14.946483	-0.045952	4.476334
226.393219	6873.083760	14.951488	-0.045949	4.473816
226.382131	6865.025221	14.956493	-0.045942	4.471276
226.261243	6857.020057	14.961498	-0.045914	4.468752
226.066357	6849.041120	14.966503	-0.045872	4.466233
225.965242	6841.015223	14.971507	-0.045848	4.463699
226.190885	6833.053188	14.976512	-0.045885	4.461185
226.006950	6825.006816	14.981517	-0.045845	4.458641
226.118343	6817.014700	14.986522	-0.045860	4.456114
226.120015	6809.015660	14.991527	-0.045855	4.453583
225.947359	6801.002731	14.996531	-0.045818	4.451046
226.062331	6793.050767	15.001536	-0.045834	4.448527
225.941166	6785.004996	15.006541	-0.045806	4.445977
226.002724	6777.029330	15.011546	-0.045812	4.443448
225.752974	6769.036892	15.016551	-0.045760	4.440910
225.762241	6761.016031	15.021555	-0.045756	4.438364
226.002128	6753.033855	15.026560	-0.045796	4.435829
225.705321	6744.952884	15.031565	-0.045735	4.433259
225.684752	6736.953185	15.036570	-0.045726	4.430714
225.680548	6728.986300	15.041575	-0.045719	4.428179
225.774930	6720.966648	15.046579	-0.045732	4.425626
225.714533	6712.998994	15.051584	-0.045715	4.423087
225.697655	6704.962831	15.056589	-0.045706	4.420525
225.701935	6697.034735	15.061594	-0.045702	4.417996
225.714107	6689.022069	15.066599	-0.045699	4.415439
225.481812	6681.005222	15.071603	-0.045650	4.412878
225.700616	6672.976119	15.076608	-0.045685	4.410313
225.505142	6664.940767	15.081613	-0.045644	4.407743
225.610876	6656.978409	15.086618	-0.045658	4.405197
225.649808	6649.022708	15.091623	-0.045660	4.402650
225.473866	6640.990436	15.096627	-0.045622	4.400077
225.511798	6633.050852	15.101632	-0.045623	4.397533
225.136736	6624.992533	15.106637	-0.045548	4.394947
225.449920	6616.967017	15.111642	-0.045601	4.392374
225.375726	6608.974297	15.116647	-0.045582	4.389807
225.214031	6600.981044	15.121651	-0.045546	4.387239
225.144996	6592.988935	15.126656	-0.045528	4.384670
225.126914	6585.020030	15.131661	-0.045519	4.382107
225.276144	6576.980952	15.136666	-0.045542	4.379521
225.278296	6569.039454	15.141671	-0.045537	4.376964
225.236638	6560.987170	15.146675	-0.045524	4.374370
225.121508	6553.035967	15.151680	-0.045497	4.371806
224.843822	6544.978413	15.156685	-0.045440	4.369205
224.915837	6537.016685	15.161690	-0.045448	4.366636
225.056229	6528.965502	15.166695	-0.045468	4.364037
224.932247	6521.013149	15.171699	-0.045440	4.361467
224.886711	6513.013781	15.176704	-0.045426	4.358880
224.886324	6505.019244	15.181709	-0.045421	4.356294
224.678079	6496.949800	15.186714	-0.045376	4.353681
224.703554	6488.893991	15.191719	-0.045376	4.351072
224.681341	6480.915264	15.196723	-0.045366	4.348486
224.690192	6472.931027	15.201728	-0.045362	4.345896
224.568319	6464.960080	15.206733	-0.045334	4.343309
224.530161	6456.971010	15.211738	-0.045322	4.340715
224.483669	6448.997486	15.216743	-0.045308	4.338125
224.508313	6440.939836	15.221747	-0.045307	4.335506
224.502692	6432.988471	15.226752	-0.045301	4.332919
224.649335	6424.917672	15.231757	-0.045323	4.330294
224.631164	6416.966561	15.236762	-0.045314	4.327704
224.597366	6408.959272	15.241767	-0.045302	4.325095
224.459295	6400.975472	15.246771	-0.045271	4.322491
224.313958	6392.971838	15.251776	-0.045239	4.319879
224.223802	6385.011042	15.256781	-0.045216	4.317279
224.325641	6376.941698	15.261786	-0.045230	4.314644
224.432062	6368.902927	15.266791	-0.045244	4.312018
224.329134	6360.915952	15.271795	-0.045220	4.309405
224.226077	6352.951042	15.276800	-0.045195	4.306798
224.095375	6344.912553	15.281805	-0.045165	4.304165
224.081729	6336.956232	15.286810	-0.045158	4.301558
223.949282	6328.952426	15.291815	-0.045128	4.298933
224.032608	6320.970151	15.296819	-0.045138	4.296315
224.208956	6312.930510	15.301824	-0.045165	4.293678
223.934988	6304.866122	15.306829	-0.045109	4.291027
223.910633	6296.900275	15.311834	-0.045099	4.288409
223.915467	6288.918640	15.316839	-0.045094	4.285784
223.704253	6280.926550	15.321843	-0.045050	4.283152
223.899703	6272.915731	15.326848	-0.045081	4.280516
223.757937	6264.962095	15.331853	-0.045049	4.277895
223.917451	6256.904229	15.336858	-0.045073	4.275240
223.890206	6248.895964	15.341863	-0.045063	4.272598
223.771449	6240.850655	15.346867	-0.045035	4.269942
223.943420	6232.916047	15.351872	-0.045062	4.267323
223.587662	6224.866333	15.356877	-0.044990	4.264659
223.604197	6216.917424	15.361882	-0.044988	4.262031
223.760677	6208.910179	15.366887	-0.045012	4.259383
223.609499	6200.943647	15.371891	-0.044978	4.256744
223.446616	6192.938171	15.376896	-0.044942	4.254090
223.709683	6184.890123	15.381901	-0.044986	4.251424
223.683054	6176.892786	15.386906	-0.044976	4.248771
223.610672	6168.891412	15.391911	-0.044957	4.246115
223.537240	6160.905449	15.396915	-0.044938	4.243462
223.495732	6152.937691	15.401920	-0.044924	4.240813
223.368311	6144.972719	15.406925	-0.044895	4.238163
223.440923	6136.945081	15.411930	-0.044904	4.235493
223.440325	6128.913374	15.416935	-0.044898	4.232818
223.421667	6120.906955	15.421939	-0.044889	4.230151
223.345034	6112.952254	15.426944	-0.044869	4.227498
223.239409	6104.882761	15.431949	-0.044844	4.224805
223.002521	6096.943011	15.436954	-0.044795	4.222152
223.192224	6088.942221	15.441959	-0.044825	4.219482
222.974542	6080.941993	15.446963	-0.044779	4.216805
223.090005	6072.969419	15.451968	-0.044795	4.214140
222.787076	6064.900944	15.456973	-0.044733	4.211437
223.080079	6056.922785	15.461978	-0.044782	4.208768
223.097022	6048.939545	15.466983	-0.044780	4.206093
222.835090	6040.924517	15.471987	-0.044726	4.203403
222.864272	6032.969738	15.476992	-0.044726	4.200734
222.931985	6024.972308	15.481997	-0.044733	4.198050
222.928991	6016.959005	15.487002	-0.044727	4.195358
222.780683	6008.845969	15.492007	-0.044694	4.192629
222.742526	6000.804311	15.497011	-0.044682	4.189923
222.817855	5992.898627	15.502016	-0.044690	4.187263
222.723158	5984.858024	15.507021	-0.044667	4.184554
222.721815	5976.919615	15.512026	-0.044662	4.181878
222.807259	5968.901061	15.517031	-0.044672	4.179175
222.572592	5960.910344	15.522035	-0.044623	4.176476
222.508251	5952.946921	15.527040	-0.044606	4.173786
222.388342	5944.871392	15.532045	-0.044578	4.171056
222.524447	5936.892224	15.537050	-0.044598	4.168359
222.643872	5928.903059	15.542055	-0.044615	4.165657
222.519720	5920.872068	15.547059	-0.044586	4.162937
222.698693	5912.920698	15.552064	-0.044614	4.160245
222.501444	5904.943248	15.557069	-0.044572	4.157538
222.529785	5896.914466	15.562074	-0.044572	4.154815
222.580907	5888.889228	15.567079	-0.044576	4.152091
222.426919	5880.857169	15.572083	-0.044542	4.149361
222.217171	5872.925179	15.577088	-0.044498	4.146662
222.211098	5864.863653	15.582093	-0.044491	4.143920
222.354982	5856.914893	15.587098	-0.044513	4.141217
221.992107	5848.926278	15.592103	-0.044440	4.138492
222.012597	5840.861447	15.597107	-0.044438	4.135743
222.068538	5832.881221	15.602112	-0.044443	4.133022
221.920703	5824.857897	15.607117	-0.044410	4.130283
221.838600	5816.897870	15.612122	-0.044390	4.127563
222.018830	5808.860370	15.617127	-0.044418	4.124819
221.952401	5800.902119	15.622131	-0.044400	4.122097
222.064699	5792.913298	15.627136	-0.044415	4.119365
222.115221	5784.973076	15.632141	-0.044420	4.116647
222.032919	5776.875487	15.637146	-0.044399	4.113871
221.730254	5768.862764	15.642151	-0.044337	4.111120
221.696145	5760.858037	15.647155	-0.044325	4.108374
221.918652	5752.875219	15.652160	-0.044361	4.105636
221.756818	5744.917889	15.657165	-0.044326	4.102900
221.678620	5736.886445	15.662170	-0.044306	4.100138
221.832509	5728.938525	15.667175	-0.044329	4.097406
221.675207	5720.902839	15.672179	-0.044294	4.094638
221.452800	5712.938639	15.677184	-0.044248	4.091891
221.568164	5704.882353	15.682189	-0.044264	4.089116
221.662706	5696.902897	15.687194	-0.044276	4.086365
221.497755	5688.949070	15.692199	-0.044240	4.083617
221.486201	5680.933990	15.697203	-0.044232	4.080848
221.683409	5672.974654	15.702208	-0.044264	4.078100
221.400071	5664.971460	15.707213	-0.044206	4.075328
221.247701	5656.922528	15.712218	-0.044172	4.072540
221.270383	5648.916188	15.717223	-0.044171	4.069767
221.422593	5640.909090	15.722227	-0.044193	4.066995
221.342966	5632.934048	15.727232	-0.044173	4.064227
221.280710	5624.928687	15.732237	-0.044156	4.061448
221.514761	5616.937185	15.737242	-0.044194	4.058676
221.335814	5608.944063	15.742247	-0.044156	4.055896
221.116734	5600.950112	15.747251	-0.044110	4.053113
221.211640	5592.934161	15.752256	-0.044122	4.050324
221.154586	5584.950748	15.757261	-0.044106	4.047543
220.985141	5576.911366	15.762266	-0.044069	4.044739
221.014129	5568.997129	15.767271	-0.044069	4.041979
220.875192	5560.920218	15.772275	-0.044038	4.039159
220.881280	5552.954469	15.777280	-0.044033	4.036377
220.891352	5544.864549	15.782285	-0.044030	4.033550
221.022215	5536.825916	15.787290	-0.044049	4.030741
221.193813	5528.882025	15.792295	-0.044075	4.027964
220.922421	5520.864078	15.797299	-0.044019	4.025152
221.040086	5512.939784	15.802304	-0.044036	4.022376
220.907489	5504.915417	15.807309	-0.044006	4.019560
220.823322	5496.946164	15.812314	-0.043985	4.016762
220.684348	5488.936077	15.817319	-0.043954	4.013947
220.727171	5480.845364	15.822323	-0.043956	4.011105
220.962585	5472.909663	15.827328	-0.043995	4.008318
220.511566	5464.917344	15.832333	-0.043905	4.005498
220.517851	5456.940192	15.837338	-0.043901	4.002689
220.495202	5448.954911	15.842343	-0.043891	3.999874
220.355394	5440.962055	15.847347	-0.043860	3.997053
220.454952	5432.941779	15.852352	-0.043873	3.994224
220.534390	5424.898919	15.857357	-0.043883	3.991385
220.432948	5416.887815	15.862362	-0.043858	3.988552
220.433081	5408.913015	15.867367	-0.043853	3.985732
220.334291	5400.907935	15.872371	-0.043829	3.982897
220.209331	5392.913357	15.877376	-0.043800	3.980064
220.129632	5384.981394	15.882381	-0.043780	3.977251
220.150911	5376.919188	15.887386	-0.043779	3.974392
220.427141	5368.928027	15.892391	-0.043825	3.971560
220.159961	5360.907793	15.897395	-0.043770	3.968707
220.346768	5352.967373	15.902400	-0.043799	3.965888
220.338121	5344.941040	15.907405	-0.043792	3.963033
220.167805	5336.948487	15.912410	-0.043755	3.960185
220.103752	5329.022313	15.917415	-0.043738	3.957360
220.020071	5320.985470	15.922419	-0.043717	3.954494
219.962136	5312.950613	15.927424	-0.043701	3.951627
219.680716	5304.930851	15.932429	-0.043643	3.948759
219.716148	5296.949461	15.937434	-0.043644	3.945908
219.804684	5288.998263	15.942439	-0.043655	3.943067
219.684433	5280.968061	15.947443	-0.043627	3.940192
219.694053	5273.041028	15.952448	-0.043624	3.937354
219.667326	5264.982165	15.957453	-0.043613	3.934466
219.627213	5256.986487	15.962458	-0.043601	3.931599
219.561269	5248.997972	15.967463	-0.043583	3.928731
219.544481	5240.973722	15.972467	-0.043574	3.925850
219.810771	5232.993087	15.977472	-0.043619	3.922987
219.766402	5225.004529	15.982477	-0.043605	3.920113
219.691531	5217.010409	15.987482	-0.043586	3.917235
219.597134	5208.996344	15.992487	-0.043563	3.914347
219.349978	5200.973616	15.997491	-0.043511	3.911451
219.359330	5192.966142	16.002496	-0.043508	3.908563
219.447009	5184.975213	16.007501	-0.043518	3.905681
219.393447	5176.970745	16.012506	-0.043503	3.902789
219.408878	5169.004024	16.017511	-0.043501	3.899909
219.291984	5161.032893	16.022515	-0.043473	3.897024
219.593740	5153.005098	16.027520	-0.043524	3.894123
219.470686	5144.960019	16.032525	-0.043496	3.891206
219.241405	5136.991245	16.037530	-0.043448	3.888313
219.375182	5128.996222	16.042535	-0.043467	3.885415
219.296455	5121.007326	16.047539	-0.043447	3.882513
219.097481	5112.972507	16.052544	-0.043405	3.879589
219.042926	5105.042463	16.057549	-0.043389	3.876704
219.100359	5096.916758	16.062554	-0.043395	3.873748
218.923400	5088.815976	16.067559	-0.043356	3.870795
218.858342	5080.873768	16.072563	-0.043339	3.867899
218.944983	5072.895012	16.077568	-0.043349	3.864990
219.014072	5064.942007	16.082573	-0.043357	3.862089
218.898335	5056.954739	16.087578	-0.043330	3.859169
218.935003	5049.020632	16.092583	-0.043332	3.856269
218.705705	5040.970761	16.097587	-0.043283	3.853319
218.880166	5032.987349	16.102592	-0.043310	3.850400
218.807548	5025.008405	16.107597	-0.043292	3.847475
218.595847	5016.960812	16.112602	-0.043247	3.844520
218.754885	5009.068726	16.117607	-0.043271	3.841627
218.695095	5001.006227	16.122611	-0.043254	3.838665
218.608791	4993.060177	16.127616	-0.043233	3.835742
218.463592	4985.050605	16.132621	-0.043201	3.832793
218.334648	4977.011579	16.137626	-0.043171	3.829832
218.616777	4969.045100	16.142631	-0.043218	3.826903
218.429424	4961.028615	16.147635	-0.043178	3.823943
218.505102	4953.087004	16.152640	-0.043187	3.821015
218.462303	4945.065334	16.157645	-0.043173	3.818052
218.318882	4937.079401	16.162650	-0.043141	3.815098
218.275835	4929.094723	16.167655	-0.043128	3.812144
218.293946	4921.017401	16.172659	-0.043126	3.809155
218.369679	4913.104817	16.177664	-0.043135	3.806226
218.303724	4905.104754	16.182669	-0.043117	3.803260
218.039038	4897.109233	16.187674	-0.043062	3.800288
218.322299	4889.126325	16.192679	-0.043110	3.797330
218.315626	4881.067623	16.197683	-0.043103	3.794336
218.102084	4873.051954	16.202688	-0.043058	3.791351
218.174795	4865.037331	16.207693	-0.043066	3.788370
218.063079	4857.027480	16.212698	-0.043040	3.785384
218.092707	4849.102581	16.217703	-0.043040	3.782431
217.930172	4841.080004	16.222707	-0.043004	3.779435
217.967202	4833.121172	16.227712	-0.043006	3.776465
217.993272	4825.127491	16.232717	-0.043005	3.773479
217.826905	4817.084250	16.237722	-0.042969	3.770468
217.820530	4809.097783	16.242727	-0.042962	3.767479
217.747414	4801.070088	16.247731	-0.042943	3.764471
217.769604	4793.129583	16.252736	-0.042942	3.761495
217.683736	4785.126314	16.257741	-0.042921	3.758491
217.592054	4777.099920	16.262746	-0.042898	3.755476
217.460501	4769.136486	16.267751	-0.042868	3.752481
217.418228	4761.076806	16.272755	-0.042855	3.749450
217.725828	4753.097183	16.277760	-0.042907	3.746454
217.740452	4745.121459	16.282765	-0.042904	3.743451
217.519746	4737.113108	16.287770	-0.042858	3.740427
217.704978	4729.143653	16.292775	-0.042887	3.737425
217.539269	4721.140724	16.297779	-0.042851	3.734400
217.596492	4713.135172	16.302784	-0.042856	3.731377
217.445038	4705.116356	16.307789	-0.042822	3.728341
217.436125	4697.151122	16.312794	-0.042815	3.725326
217.539315	4689.193409	16.317799	-0.042829	3.722315
217.369966	4681.164096	16.322803	-0.042792	3.719267
217.339072	4673.240290	16.327808	-0.042781	3.716260
217.228130	4665.162878	16.332813	-0.042755	3.713191
217.243202	4657.062683	16.337818	-0.042752	3.710113
217.338119	4649.129778	16.342823	-0.042765	3.707098
217.215504	4641.138757	16.347827	-0.042737	3.704054
217.193656	4633.171538	16.352832	-0.042727	3.701018
216.904021	4625.197323	16.357837	-0.042668	3.697971
217.168145	4617.180315	16.362842	-0.042712	3.694919
217.194694	4609.199384	16.367847	-0.042711	3.691872
217.060459	4601.182596	16.372851	-0.042681	3.688804
217.073084	4593.197882	16.377856	-0.042678	3.685750
217.061063	4585.252402	16.382861	-0.042670	3.682708
216.824482	4577.206309	16.387866	-0.042621	3.679619
216.852037	4569.297522	16.392871	-0.042620	3.676587
216.685242	4561.252987	16.397875	-0.042584	3.673495
216.662290	4553.212124	16.402880	-0.042574	3.670406
216.503305	4545.234311	16.407885	-0.042539	3.667335
216.556826	4537.201019	16.412890	-0.042544	3.664246
216.774729	4529.234642	16.417895	-0.042579	3.661183
216.792354	4521.228554	16.422899	-0.042577	3.658098
216.703374	4513.246205	16.427904	-0.042555	3.655017
216.666566	4505.242003	16.432909	-0.042543	3.651926
216.594556	4497.216327	16.437914	-0.042524	3.648823
216.529166	4489.256776	16.442919	-0.042506	3.645743
216.450107	4481.269453	16.447923	-0.042486	3.642649
216.515327	4473.276552	16.452928	-0.042493	3.639555
216.542039	4465.327711	16.457933	-0.042493	3.636474
216.377787	4457.260569	16.462938	-0.042457	3.633339
216.445891	4449.237280	16.467943	-0.042464	3.630225
216.283501	4441.244214	16.472947	-0.042428	3.627113
216.321755	4433.246407	16.477952	-0.042430	3.624003
216.408886	4425.280866	16.482957	-0.042441	3.620904
216.268030	4417.295765	16.487962	-0.042409	3.617788
216.210344	4409.313326	16.492967	-0.042393	3.614673
215.952513	4401.312836	16.497971	-0.042340	3.611542
216.073275	4393.297252	16.502976	-0.042357	3.608414
215.885990	4385.324919	16.507981	-0.042317	3.605291
215.844554	4377.344363	16.512986	-0.042304	3.602166
215.980620	4369.346074	16.517991	-0.042323	3.599037
215.843421	4361.401405	16.522995	-0.042293	3.595918
215.864865	4353.367166	16.528000	-0.042291	3.592765
215.887139	4345.350243	16.533005	-0.042290	3.589617
215.766199	4337.352323	16.538010	-0.042262	3.586470
215.771775	4329.383216	16.543015	-0.042258	3.583334
215.783566	4321.389731	16.548019	-0.042254	3.580187
215.821539	4313.419572	16.553024	-0.042256	3.577046
215.675823	4305.427149	16.558029	-0.042224	3.573889
215.694131	4297.383178	16.563034	-0.042222	3.570713
215.702802	4289.431561	16.568039	-0.042218	3.567571
215.436904	4281.400730	16.573043	-0.042163	3.564386
215.519653	4273.437294	16.578048	-0.042173	3.561236
215.607651	4265.430084	16.583053	-0.042184	3.558066
215.317445	4257.450266	16.588058	-0.042125	3.554892
215.266185	4249.375763	16.593063	-0.042110	3.551685
215.270787	4241.340529	16.598067	-0.042105	3.548493
215.369648	4233.354893	16.603072	-0.042118	3.545320
215.440166	4225.405154	16.608077	-0.042126	3.542157
215.302584	4217.386539	16.613082	-0.042095	3.538959
215.440035	4209.423313	16.618087	-0.042115	3.535787
215.385231	4201.433274	16.623091	-0.042099	3.532597
215.284138	4193.442284	16.628096	-0.042075	3.529401
215.130153	4185.457930	16.633101	-0.042041	3.526204
215.102707	4177.436140	16.638106	-0.042031	3.522993
215.273337	4169.465720	16.643111	-0.042057	3.519805
215.201335	4161.501618	16.648115	-0.042038	3.516610
215.167401	4153.484319	16.653120	-0.042027	3.513391
215.068096	4145.484094	16.658125	-0.042003	3.510175
215.062832	4137.483204	16.663130	-0.041996	3.506958
215.145450	4129.508438	16.668135	-0.042006	3.503751
215.112070	4121.494176	16.673139	-0.041995	3.500522
214.741155	4113.579426	16.678144	-0.041920	3.497320
214.905365	4105.560697	16.683149	-0.041946	3.494089
214.589368	4097.535931	16.688154	-0.041881	3.490838
214.645225	4089.572190	16.693159	-0.041886	3.487620
214.756385	4081.534309	16.698163	-0.041902	3.484371
214.775270	4073.561240	16.703168	-0.041900	3.481142
214.805349	4065.616231	16.708173	-0.041900	3.477922
214.695557	4057.588151	16.713178	-0.041874	3.474661
214.628560	4049.571179	16.718183	-0.041856	3.471402
214.570512	4041.568732	16.723187	-0.041840	3.468147
214.576594	4033.567177	16.728192	-0.041836	3.464891
214.463625	4025.597232	16.733197	-0.041809	3.461641
214.418863	4017.601036	16.738202	-0.041796	3.458379
214.464143	4009.620461	16.743207	-0.041799	3.455124
214.492882	4001.616639	16.748211	-0.041799	3.451856
214.401357	3993.620188	16.753216	-0.041776	3.448583
214.388795	3985.634891	16.758221	-0.041769	3.445315
214.196071	3977.648198	16.763226	-0.041727	3.442037
214.319762	3969.667805	16.768231	-0.041745	3.438769
214.221041	3961.672797	16.773235	-0.041721	3.435484
214.226113	3953.667883	16.778240	-0.041717	3.432195
214.246865	3945.640521	16.783245	-0.041715	3.428895
214.105094	3937.662290	16.788250	-0.041683	3.425607
213.927835	3929.725767	16.793255	-0.041645	3.422331
213.767723	3921.710770	16.798259	-0.041610	3.419020
213.972682	3913.730099	16.803264	-0.041643	3.415732
214.003457	3905.709542	16.808269	-0.041643	3.412419
213.687225	3897.721845	16.813274	-0.041579	3.409105
213.905223	3889.720915	16.818279	-0.041614	3.405800
213.783465	3881.754527	16.823283	-0.041586	3.402494
213.668538	3873.782583	16.828288	-0.041559	3.399183
213.864545	3865.792373	16.833293	-0.041590	3.395872
213.832470	3857.711929	16.838298	-0.041579	3.392513
213.820317	3849.699333	16.843303	-0.041571	3.389179
213.771318	3841.720226	16.848307	-0.041557	3.385854
213.827054	3833.779788	16.853312	-0.041562	3.382546
213.608559	3825.791103	16.858317	-0.041516	3.379205
213.510096	3817.834581	16.863322	-0.041492	3.375878
213.524021	3809.811438	16.868327	-0.041489	3.372524
213.354706	3801.779874	16.873331	-0.041452	3.369157
213.440882	3793.821689	16.878336	-0.041463	3.365826
213.414455	3785.856457	16.883341	-0.041452	3.362485
213.496085	3777.827418	16.888346	-0.041462	3.359117
213.335357	3769.909728	16.893351	-0.041427	3.355784
213.275740	3761.853996	16.898355	-0.041410	3.352394
213.138735	3753.865029	16.903360	-0.041380	3.349025
213.241644	3745.875189	16.908365	-0.041393	3.345662
212.993208	3737.896542	16.913370	-0.041342	3.342286
213.070767	3729.926468	16.918375	-0.041351	3.338923
213.113182	3721.922436	16.923379	-0.041353	3.335541
213.035319	3713.914920	16.928384	-0.041333	3.332150
212.908571	3705.918415	16.933389	-0.041304	3.328758
212.971062	3697.908327	16.938394	-0.041311	3.325364
213.136812	3689.950955	16.943399	-0.041336	3.321992
212.980504	3681.975697	16.948403	-0.041302	3.318598
212.893424	3673.993011	16.953408	-0.041280	3.315199
212.923832	3665.964891	16.958413	-0.041280	3.311782
212.668388	3657.963881	16.963418	-0.041227	3.308362
212.692418	3649.991705	16.968423	-0.041227	3.304962
212.655129	3642.027359	16.973427	-0.041214	3.301559
212.530351	3634.025800	16.978432	-0.041186	3.298133
212.585607	3626.061672	16.983437	-0.041190	3.294727
212.469046	3618.021423	16.988442	-0.041163	3.291277
212.532153	3610.041140	16.993447	-0.041170	3.287857
212.495513	3602.041073	16.998451	-0.041158	3.284421
212.564908	3594.087000	17.003456	-0.041165	3.281005
212.755910	3586.115649	17.008461	-0.041195	3.277583
212.416646	3578.132611	17.013466	-0.041127	3.274132
212.477983	3570.107930	17.018471	-0.041133	3.270675
212.362914	3562.105637	17.023475	-0.041106	3.267216
212.203341	3554.112335	17.028480	-0.041071	3.263757
211.873374	3546.164128	17.033485	-0.041004	3.260306
212.103432	3538.142081	17.038490	-0.041041	3.256842
212.210542	3530.157055	17.043495	-0.041056	3.253385
211.998240	3522.146637	17.048499	-0.041011	3.249901
212.034765	3514.178675	17.053504	-0.041013	3.246441
212.249887	3506.179690	17.058509	-0.041047	3.242972
212.222216	3498.180871	17.063514	-0.041037	3.239489
212.097880	3490.262676	17.068519	-0.041008	3.236034
211.949731	3482.182832	17.073523	-0.040975	3.232503
211.936784	3474.161432	17.078528	-0.040967	3.228999
212.046405	3466.170111	17.083533	-0.040982	3.225510
211.904683	3458.215232	17.088538	-0.040951	3.222023
211.982318	3450.253414	17.093543	-0.040960	3.218538
211.738675	3442.256446	17.098547	-0.040909	3.215020
211.705548	3434.263415	17.103552	-0.040897	3.211509
211.895589	3426.282185	17.108557	-0.040927	3.208009
211.581490	3418.294932	17.113562	-0.040864	3.204481
211.682441	3410.359400	17.118567	-0.040877	3.200989
211.784077	3402.340437	17.123571	-0.040891	3.197457
211.720298	3394.347468	17.128576	-0.040873	3.193925
211.527458	3386.371463	17.133581	-0.040832	3.190392
211.428362	3378.348881	17.138586	-0.040808	3.186838
211.613301	3370.354557	17.143591	-0.040837	3.183304
211.318784	3362.416494	17.148595	-0.040777	3.179772
211.313761	3354.425093	17.153600	-0.040771	3.176223
211.406091	3346.422707	17.158605	-0.040782	3.172671
211.201891	3338.395495	17.163610	-0.040739	3.169090
211.252307	3330.436853	17.168615	-0.040743	3.165547
211.206626	3322.467740	17.173619	-0.040729	3.161991
211.146658	3314.474762	17.178624	-0.040713	3.158420
211.215039	3306.492315	17.183629	-0.040720	3.154855
211.160692	3298.457625	17.188634	-0.040704	3.151257
211.161854	3290.473378	17.193639	-0.040699	3.147680
211.148622	3282.488488	17.198643	-0.040691	3.144098
210.973638	3274.508439	17.203648	-0.040653	3.140507
211.037905	3266.563350	17.208653	-0.040660	3.136938
210.824664	3258.529142	17.213658	-0.040615	3.133313
210.808970	3250.555464	17.218663	-0.040607	3.129720
210.658575	3242.589761	17.223667	-0.040573	3.126120
210.720531	3234.582545	17.228672	-0.040579	3.122506
210.963432	3226.611449	17.233677	-0.040619	3.118913
210.751899	3218.658126	17.238682	-0.040575	3.115303
210.757017	3210.658783	17.243687	-0.040570	3.111679
210.761185	3202.635161	17.248691	-0.040565	3.108038
210.455541	3194.665012	17.253696	-0.040503	3.104404
210.519989	3186.694668	17.258701	-0.040510	3.100782
210.425859	3178.709114	17.263706	-0.040487	3.097142
210.375119	3170.729315	17.268711	-0.040472	3.093502
210.445368	3162.684515	17.273715	-0.040480	3.089834
210.451864	3154.729429	17.278720	-0.040476	3.086199
210.369445	3146.773623	17.283725	-0.040455	3.082556
210.497706	3138.748663	17.288730	-0.040473	3.078886
210.616396	3130.782492	17.293735	-0.040490	3.075238
210.303196	3122.733107	17.298739	-0.040426	3.071528
210.222796	3114.750627	17.303744	-0.040406	3.067855
210.389670	3106.760602	17.308749	-0.040432	3.064186
210.226558	3098.794233	17.313754	-0.040396	3.060508
210.231712	3090.840547	17.318759	-0.040392	3.056839
210.166838	3082.861053	17.323763	-0.040374	3.053150
210.127761	3074.838651	17.328768	-0.040361	3.049438
210.033562	3066.906530	17.333773	-0.040339	3.045761
209.888049	3058.923384	17.338778	-0.040306	3.042053
210.268775	3050.915696	17.343783	-0.040372	3.038355
210.079314	3042.962648	17.348787	-0.040331	3.034650
209.940584	3034.942381	17.353792	-0.040300	3.030912
209.970743	3026.970749	17.358797	-0.040300	3.027200
209.864577	3018.976953	17.363802	-0.040275	3.023466
209.880015	3011.023133	17.368807	-0.040272	3.019753
209.610218	3003.062260	17.373811	-0.040217	3.016017
209.571758	2995.024465	17.378816	-0.040204	3.012252
209.603123	2987.041318	17.383821	-0.040205	3.008512
209.650499	2979.034488	17.388826	-0.040208	3.004756
209.772821	2971.082191	17.393831	-0.040225	3.001026
209.543928	2963.141043	17.398835	-0.040177	2.997278
209.428029	2955.143670	17.403840	-0.040150	2.993505
209.643414	2947.103431	17.408845	-0.040185	2.989723
209.429618	2939.126805	17.413850	-0.040140	2.985945
209.367784	2931.173236	17.418855	-0.040123	2.982181
209.233983	2923.193270	17.423859	-0.040093	2.978396
209.348234	2915.189110	17.428864	-0.040109	2.974607
209.420556	2907.195637	17.433869	-0.040117	2.970816
209.054245	2899.234436	17.438874	-0.040043	2.967014
209.012326	2891.279589	17.443879	-0.040030	2.963226
209.246332	2883.252199	17.448883	-0.040068	2.959412
208.964623	2875.341001	17.453888	-0.040010	2.955623
209.139601	2867.307166	17.458893	-0.040038	2.951794
209.079494	2859.298021	17.463898	-0.040021	2.947960
209.052662	2851.325034	17.468903	-0.040011	2.944139
208.996717	2843.346708	17.473907	-0.039995	2.940310
208.795184	2835.406992	17.478912	-0.039952	2.936486
208.966954	2827.417569	17.483917	-0.039979	2.932653
208.882073	2819.382939	17.488922	-0.039957	2.928780
208.938948	2811.424366	17.493927	-0.039963	2.924946
208.810833	2803.481606	17.498931	-0.039933	2.921105
208.744135	2795.491635	17.503936	-0.039916	2.917239
208.795634	2787.478023	17.508941	-0.039920	2.913363
208.866557	2779.405324	17.513946	-0.039928	2.909454
208.593557	2771.468814	17.518951	-0.039871	2.905587
208.508132	2763.526131	17.523955	-0.039850	2.901722
208.678879	2755.525960	17.528960	-0.039876	2.897838
208.632658	2747.561133	17.533965	-0.039863	2.893954
208.321844	2739.575045	17.538970	-0.039799	2.890041
208.453236	2731.598607	17.543975	-0.039818	2.886150
208.613077	2723.634146	17.548979	-0.039843	2.882262
208.459759	2715.672662	17.553984	-0.039809	2.878353
208.332233	2707.711559	17.558989	-0.039780	2.874440
208.120614	2699.707921	17.563994	-0.039735	2.870497
208.179061	2691.707905	17.568999	-0.039740	2.866564
208.035809	2683.744688	17.574003	-0.039708	2.862633
208.158185	2675.732203	17.579008	-0.039726	2.858687
208.134916	2667.781888	17.584013	-0.039716	2.854759
208.049321	2659.790292	17.589018	-0.039695	2.850801
207.982361	2651.826626	17.594023	-0.039677	2.846852
207.914484	2643.859055	17.599027	-0.039659	2.842896
207.872262	2635.878343	17.604032	-0.039646	2.838929
207.884770	2627.927040	17.609037	-0.039643	2.834974
207.978702	2619.871071	17.614042	-0.039655	2.830966
207.797638	2611.910399	17.619047	-0.039616	2.826985
207.671240	2603.944795	17.624051	-0.039587	2.822998
207.756417	2595.953794	17.629056	-0.039597	2.819006
207.819273	2587.992822	17.634061	-0.039604	2.815021
207.584564	2580.014492	17.639066	-0.039554	2.811005
207.736570	2572.039171	17.644071	-0.039577	2.807007
207.758578	2564.053541	17.649075	-0.039576	2.802990
207.520174	2556.093956	17.654080	-0.039526	2.798966
207.628975	2548.123692	17.659085	-0.039541	2.794951
207.306760	2540.135147	17.664090	-0.039476	2.790896
207.413561	2532.144944	17.669095	-0.039490	2.786858
207.243766	2524.186737	17.674099	-0.039453	2.782815
207.185980	2516.214228	17.679104	-0.039437	2.778766
207.154136	2508.247276	17.684109	-0.039426	2.774715
207.165985	2500.222512	17.689114	-0.039423	2.770631
207.182000	2492.272123	17.694119	-0.039420	2.766579
207.161721	2484.294849	17.699123	-0.039411	2.762506
206.959185	2476.345882	17.704128	-0.039368	2.758430
207.157968	2468.348147	17.709133	-0.039400	2.754347
207.037421	2460.290286	17.714138	-0.039372	2.750207
207.175465	2452.322225	17.719143	-0.039392	2.746124
206.938818	2444.384769	17.724147	-0.039343	2.742027
206.779985	2436.427075	17.729152	-0.039308	2.737919
207.117229	2428.421352	17.734157	-0.039365	2.733809
206.969722	2420.431334	17.739162	-0.039332	2.729672
206.851440	2412.489826	17.744167	-0.039305	2.725556
206.990073	2404.521927	17.749171	-0.039326	2.721436
206.963961	2396.545413	17.754176	-0.039315	2.717294
206.881221	2388.599249	17.759181	-0.039295	2.713159
206.679173	2380.611820	17.764186	-0.039252	2.708988
206.644221	2372.646075	17.769191	-0.039240	2.704833
206.590794	2364.678082	17.774195	-0.039224	2.700669
206.347269	2356.729780	17.779200	-0.039174	2.696496
206.600445	2348.715571	17.784205	-0.039215	2.692315
206.631354	2340.701855	17.789210	-0.039216	2.688112
206.445571	2332.775544	17.794215	-0.039176	2.683936
206.548081	2324.787627	17.799219	-0.039189	2.679738
206.512511	2316.844898	17.804224	-0.039178	2.675550
206.321028	2308.855571	17.809229	-0.039136	2.671320
206.390850	2300.843071	17.814234	-0.039144	2.667088
206.404658	2292.887186	17.819239	-0.039141	2.662875
206.259368	2284.937429	17.824243	-0.039109	2.658649
206.005797	2276.973709	17.829248	-0.039056	2.654401
206.273981	2268.968058	17.834253	-0.039101	2.650159
206.101206	2261.000487	17.839258	-0.039063	2.645901
206.055490	2253.056231	17.844263	-0.039049	2.641657
205.916704	2245.108507	17.849267	-0.039018	2.637398
205.926049	2237.114086	17.854272	-0.039015	2.633117
205.899612	2229.136785	17.859277	-0.039004	2.628835
205.794986	2221.152261	17.864282	-0.038979	2.624538
205.909051	2213.190015	17.869287	-0.038995	2.620260
205.787702	2205.237785	17.874291	-0.038967	2.615965
205.772379	2197.236697	17.879296	-0.038959	2.611644
205.673187	2189.278901	17.884301	-0.038935	2.607333
205.537447	2181.325344	17.889306	-0.038905	2.603015
205.683475	2173.355359	17.894311	-0.038926	2.598700
205.647430	2165.383691	17.899315	-0.038914	2.594364
205.545615	2157.224780	17.904320	-0.038890	2.589914
205.447708	2149.296497	17.909325	-0.038866	2.585583
205.249801	2141.376125	17.914330	-0.038824	2.581243
205.545685	2133.398254	17.919335	-0.038874	2.576897
205.662082	2125.428385	17.924339	-0.038890	2.572536
205.438225	2117.481930	17.929344	-0.038843	2.568157
205.420581	2109.533598	17.934349	-0.038835	2.563784
205.563554	2101.564642	17.939354	-0.038856	2.559403
205.220704	2093.663175	17.944359	-0.038787	2.555017
205.305188	2085.671873	17.949363	-0.038797	2.550605
205.206547	2077.687491	17.954368	-0.038773	2.546176
205.202877	2069.747695	17.959373	-0.038767	2.541770
205.012144	2061.787423	17.964378	-0.038726	2.537333
205.021023	2053.817662	17.969383	-0.038723	2.532896
204.963157	2045.837952	17.974387	-0.038706	2.528441
205.010428	2037.849938	17.979392	-0.038710	2.523981
205.130434	2029.904297	17.984397	-0.038727	2.519543
204.907320	2021.984944	17.989402	-0.038680	2.515086
204.833270	2013.973676	17.994407	-0.038661	2.510581
204.849551	2005.995954	17.999411	-0.038658	2.506093
204.886819	1998.006561	18.004416	-0.038660	2.501592
204.830111	1990.070174	18.009421	-0.038644	2.497105
204.645670	1982.116092	18.014426	-0.038604	2.492592
204.567478	1974.150372	18.019431	-0.038584	2.488071
204.521920	1966.187246	18.024435	-0.038571	2.483546
204.530526	1958.228050	18.029440	-0.038567	2.479019
204.464531	1950.295283	18.034445	-0.038549	2.474493
204.653638	1942.277973	18.039450	-0.038579	2.469930
204.411796	1934.346347	18.044455	-0.038529	2.465375
204.184302	1926.413497	18.049459	-0.038481	2.460812
204.116650	1918.441697	18.054464	-0.038463	2.456230
204.296982	1910.461233	18.059469	-0.038491	2.451653
204.272406	1902.476187	18.064474	-0.038481	2.447049
204.085647	1894.551819	18.069479	-0.038441	2.442460
204.022176	1886.609230	18.074483	-0.038424	2.437860
203.986848	1878.601260	18.079488	-0.038412	2.433217
204.100938	1870.579454	18.084493	-0.038428	2.428567
203.818423	1862.636658	18.089498	-0.038370	2.423925
204.079992	1854.672481	18.094503	-0.038413	2.419302
204.084928	1846.721352	18.099507	-0.038409	2.414659
203.966024	1838.751589	18.104512	-0.038381	2.409987
203.872814	1830.821330	18.109517	-0.038359	2.405330
203.729474	1822.890859	18.114522	-0.038326	2.400660
203.809863	1814.931738	18.119527	-0.038336	2.395982
203.916513	1806.951271	18.124531	-0.038351	2.391284
203.519586	1799.020816	18.129536	-0.038271	2.386567
203.645433	1791.049392	18.134541	-0.038289	2.381857
203.531859	1783.102647	18.139546	-0.038263	2.377134
203.549124	1775.135809	18.144551	-0.038261	2.372400
203.358779	1767.199446	18.149555	-0.038220	2.367658
203.337637	1759.228853	18.154560	-0.038211	2.362899
203.430682	1751.284201	18.159565	-0.038223	2.358156
203.167246	1743.346920	18.164570	-0.038168	2.353378
203.101026	1735.358967	18.169575	-0.038150	2.348577
203.267990	1727.365360	18.174579	-0.038176	2.343781
203.216364	1719.421808	18.179584	-0.038161	2.338987
203.178844	1711.490066	18.184589	-0.038149	2.334192
203.253226	1703.491912	18.189594	-0.038157	2.329357
203.023193	1695.580857	18.194599	-0.038109	2.324538
203.055311	1687.640809	18.199603	-0.038110	2.319714
203.059579	1679.693406	18.204608	-0.038105	2.314873
202.899261	1671.733293	18.209613	-0.038070	2.310001
202.798350	1663.776574	18.214618	-0.038046	2.305125
202.895647	1655.814621	18.219623	-0.038059	2.300252
202.985420	1647.861612	18.224627	-0.038070	2.295374
202.830299	1639.910019	18.229632	-0.038036	2.290465
202.821413	1631.970819	18.234637	-0.038029	2.285566
202.762472	1624.017718	18.239642	-0.038012	2.280643
202.812786	1616.080802	18.244647	-0.038016	2.275730
202.589534	1608.077573	18.249651	-0.037969	2.270741
202.427598	1600.119653	18.254656	-0.037934	2.265774
202.592735	1592.168871	18.259661	-0.037959	2.260829
202.532689	1584.224507	18.264666	-0.037943	2.255858
202.363740	1576.279242	18.269671	-0.037906	2.250866
202.445939	1568.323152	18.274675	-0.037916	2.245878
202.424909	1560.388176	18.279680	-0.037907	2.240883
202.443287	1552.470082	18.284685	-0.037905	2.235891
202.377522	1544.494344	18.289690	-0.037887	2.230843
202.309818	1536.548281	18.294695	-0.037869	2.225803
202.319624	1528.616982	18.299699	-0.037866	2.220768
202.169763	1520.685666	18.304704	-0.037832	2.215707
202.224543	1512.730558	18.309709	-0.037837	2.210638
202.000922	1504.791423	18.314714	-0.037790	2.205542
202.013569	1496.863955	18.319719	-0.037787	2.200463
202.135843	1488.914269	18.324723	-0.037805	2.195368
202.029920	1480.929736	18.329728	-0.037780	2.190218
201.722264	1473.014135	18.334733	-0.037717	2.185082
201.939085	1465.050157	18.339738	-0.037752	2.179950
201.673943	1457.143905	18.344743	-0.037697	2.174800
201.729055	1449.179801	18.349747	-0.037702	2.169629
201.581310	1441.231698	18.354752	-0.037669	2.164438
201.601216	1433.326349	18.359757	-0.037668	2.159277
201.555983	1425.378670	18.364762	-0.037654	2.154070
201.332627	1417.435073	18.369767	-0.037607	2.148837
201.343479	1409.496623	18.374771	-0.037604	2.143616
201.384229	1401.545298	18.379776	-0.037606	2.138377
201.365353	1393.612305	18.384781	-0.037597	2.133131
201.314057	1385.660427	18.389786	-0.037582	2.127857
201.486001	1377.700125	18.394791	-0.037609	2.122586
201.456880	1369.801322	18.399795	-0.037598	2.117323
201.266502	1361.836853	18.404800	-0.037557	2.111987
201.130274	1353.872925	18.409805	-0.037526	2.106644
200.958508	1345.961382	18.414810	-0.037489	2.101318
200.840304	1338.053664	18.419815	-0.037462	2.095987
200.975219	1330.085007	18.424819	-0.037482	2.090626
200.860764	1322.146629	18.429824	-0.037455	2.085247
200.901424	1314.236121	18.434829	-0.037457	2.079889
200.846224	1306.314271	18.439834	-0.037441	2.074499
200.858282	1298.360662	18.444839	-0.037438	2.069080
200.932886	1290.418946	18.449843	-0.037447	2.063662
200.626352	1282.538526	18.454848	-0.037385	2.058233
200.838366	1274.589297	18.459853	-0.037419	2.052794
200.754140	1266.648265	18.464858	-0.037398	2.047317
200.527874	1258.757517	18.469863	-0.037350	2.041845
200.546632	1250.832222	18.474867	-0.037348	2.036360
200.376215	1242.879532	18.479872	-0.037311	2.030821
200.444078	1234.932544	18.484877	-0.037318	2.025296
200.263638	1227.032884	18.489882	-0.037280	2.019763
200.264141	1219.109753	18.494887	-0.037274	2.014217
200.463557	1211.140773	18.499891	-0.037306	2.008644
200.278660	1203.238509	18.504896	-0.037266	2.003063
200.299921	1195.331327	18.509901	-0.037265	1.997484
200.257165	1187.398225	18.514906	-0.037252	1.991865
200.089517	1179.489193	18.519911	-0.037215	1.986233
200.193466	1171.550409	18.524915	-0.037229	1.980593
200.058367	1163.649262	18.529920	-0.037199	1.974938
199.840116	1155.751677	18.534925	-0.037153	1.969261
199.708105	1147.836762	18.539930	-0.037123	1.963564
199.773827	1139.913987	18.544935	-0.037130	1.957866
199.951560	1131.949914	18.549939	-0.037157	1.952134
199.695329	1124.020197	18.554944	-0.037104	1.946362
199.711344	1116.103509	18.559949	-0.037102	1.940613
199.841156	1108.167012	18.564954	-0.037121	1.934844
199.664533	1100.262263	18.569959	-0.037083	1.929048
199.448022	1092.387621	18.574963	-0.037037	1.923252
199.406832	1084.471370	18.579968	-0.037024	1.917427
199.461590	1076.556208	18.584973	-0.037029	1.911596
199.174358	1068.666143	18.589978	-0.036970	1.905727
199.257554	1060.735798	18.594983	-0.036980	1.899852
199.300726	1052.826117	18.599987	-0.036983	1.893969
198.923125	1044.928099	18.604992	-0.036907	1.888029
199.173367	1037.000219	18.609997	-0.036948	1.882120
199.202498	1029.104972	18.615002	-0.036949	1.876191
199.008067	1021.194509	18.620007	-0.036907	1.870206
198.966055	1013.284560	18.625011	-0.036894	1.864220
198.917512	1005.384581	18.630016	-0.036880	1.858221
198.883255	997.482331	18.635021	-0.036868	1.852203
198.797851	989.574617	18.640026	-0.036847	1.846155
198.823996	981.668195	18.645031	-0.036846	1.840102
198.853997	973.786325	18.650035	-0.036846	1.834047
198.682076	965.878037	18.655040	-0.036809	1.827928
198.500408	958.014763	18.660045	-0.036770	1.821823
198.446418	950.106678	18.665050	-0.036755	1.815677
198.443797	942.196431	18.670055	-0.036749	1.809515
198.174711	934.346543	18.675059	-0.036693	1.803346
198.139909	926.450267	18.680064	-0.036682	1.797149
198.203483	918.493690	18.685069	-0.036688	1.790894
198.083572	910.590932	18.690074	-0.036660	1.784638
198.094037	902.703349	18.695079	-0.036657	1.778388
198.154548	894.802147	18.700083	-0.036663	1.772111
198.056455	886.912171	18.705088	-0.036639	1.765801
197.904564	879.067008	18.710093	-0.036606	1.759497
197.781158	871.197342	18.715098	-0.036577	1.753155
197.730927	863.293021	18.720103	-0.036563	1.746771
197.770123	855.407629	18.725107	-0.036565	1.740390
197.821551	847.515796	18.730112	-0.036569	1.733982
197.959934	839.604241	18.735117	-0.036589	1.727545
197.776908	831.765852	18.740122	-0.036550	1.721103
197.531259	823.930208	18.745127	-0.036499	1.714630
197.602078	816.010830	18.750131	-0.036507	1.708105
197.615489	808.116161	18.755136	-0.036504	1.701568
197.561624	800.269321	18.760141	-0.036489	1.695037
197.639158	792.366424	18.765146	-0.036498	1.688451
197.569340	784.507889	18.770151	-0.036480	1.681857
197.275464	776.701260	18.775155	-0.036420	1.675251
197.129449	768.827485	18.780160	-0.036387	1.668581
197.316553	760.925914	18.785165	-0.036417	1.661906
197.321088	753.059448	18.790170	-0.036412	1.655210
197.204774	745.199351	18.795175	-0.036385	1.648475
197.354972	737.325483	18.800179	-0.036408	1.641737
197.187041	729.493303	18.805184	-0.036371	1.634963
196.883904	721.611630	18.810189	-0.036310	1.628100
196.969310	713.734774	18.815194	-0.036320	1.621266
196.954937	705.881440	18.820199	-0.036312	1.614409
196.833986	698.043860	18.825203	-0.036284	1.607522
196.723161	690.205919	18.830208	-0.036258	1.600606
196.904865	682.342528	18.835213	-0.036287	1.593680
196.784028	674.498438	18.840218	-0.036259	1.586697
196.623894	666.676759	18.845223	-0.036224	1.579698
196.735813	658.814998	18.850227	-0.036240	1.572671
196.598991	650.975922	18.855232	-0.036209	1.565596
196.704554	643.144860	18.860237	-0.036223	1.558532
196.718635	635.290516	18.865242	-0.036221	1.551402
196.641815	627.445611	18.870247	-0.036201	1.544233
196.480192	619.652601	18.875251	-0.036166	1.537066
196.305328	611.829018	18.880256	-0.036128	1.529836
196.354182	603.998565	18.885261	-0.036132	1.522598
196.188580	596.204788	18.890266	-0.036096	1.515327
196.184187	588.359217	18.895271	-0.036089	1.507998
196.178406	580.543470	18.900275	-0.036083	1.500660
196.146431	572.718972	18.905280	-0.036072	1.493274
196.018479	564.916805	18.910285	-0.036043	1.485857
196.152540	557.094871	18.915290	-0.036062	1.478426
195.926265	549.277937	18.920295	-0.036015	1.470905
195.913683	541.459111	18.925299	-0.036007	1.463377
195.733600	533.674492	18.930304	-0.035969	1.455817
195.821614	525.845961	18.935309	-0.035980	1.448217
195.604239	518.079801	18.940314	-0.035934	1.440589
195.534890	510.300738	18.945319	-0.035916	1.432932
195.548045	502.493992	18.950323	-0.035913	1.425220
195.505967	494.707949	18.955328	-0.035900	1.417477
195.431707	486.928728	18.960333	-0.035881	1.409693
195.469370	479.137021	18.965338	-0.035883	1.401872
195.238555	471.397107	18.970343	-0.035835	1.394015
195.296540	463.585167	18.975347	-0.035840	1.386088
194.973504	455.861105	18.980352	-0.035775	1.378141
195.107405	448.062519	18.985357	-0.035794	1.370150
194.944672	440.317147	18.990362	-0.035759	1.362115
194.910640	432.560165	18.995367	-0.035747	1.354043
194.931920	424.782233	19.000371	-0.035746	1.345910
194.761282	417.057502	19.005376	-0.035709	1.337750
194.554270	409.328327	19.010381	-0.035665	1.329529
194.529658	401.582066	19.015386	-0.035655	1.321271
194.424640	393.810456	19.020391	-0.035631	1.312919
194.437573	385.973453	19.025395	-0.035628	1.304464
194.330525	378.261686	19.030400	-0.035603	1.296068
194.313756	370.538994	19.035405	-0.035594	1.287623
194.134282	362.853525	19.040410	-0.035556	1.279132
193.926294	355.163597	19.045415	-0.035512	1.270575
193.980372	347.442853	19.050419	-0.035517	1.261974
194.164759	339.699733	19.055424	-0.035546	1.253314
193.940177	332.035342	19.060429	-0.035499	1.244604
193.671773	324.398305	19.065434	-0.035444	1.235856
193.625610	316.667942	19.070439	-0.035430	1.226981
193.806618	308.965907	19.075443	-0.035458	1.218119
193.416966	301.337380	19.080448	-0.035381	1.209165
193.535160	293.643797	19.085453	-0.035397	1.200169
193.653997	285.953462	19.090458	-0.035414	1.191109
193.411729	278.330740	19.095463	-0.035364	1.181987
193.403591	270.687006	19.100467	-0.035357	1.172817
193.424444	263.023731	19.105472	-0.035356	1.163556
193.254056	255.422135	19.110477	-0.035319	1.154257
192.979298	247.793108	19.115482	-0.035263	1.144826
192.932784	240.166569	19.120487	-0.035249	1.135369
193.007982	232.530479	19.125491	-0.035258	1.125846
192.730915	224.973712	19.130496	-0.035201	1.116266
192.680709	217.365283	19.135501	-0.035187	1.106586
192.540957	209.798150	19.140506	-0.035156	1.096855
192.224225	202.248864	19.145511	-0.035092	1.087020
192.211035	194.686341	19.150515	-0.035084	1.077146
192.116059	187.106967	19.155520	-0.035061	1.067140
192.068242	179.560930	19.160525	-0.035047	1.057094
191.827733	172.038380	19.165530	-0.034997	1.046939
191.794080	164.513507	19.170535	-0.034986	1.036730
191.707416	156.999552	19.175539	-0.034965	1.026421
191.360546	149.539361	19.180544	-0.034895	1.016020
190.950115	142.095269	19.185549	-0.034814	1.005518
190.594470	134.656985	19.190554	-0.034743	0.994927
189.995768	127.222957	19.195559	-0.034626	0.984167
189.554233	119.818220	19.200563	-0.034539	0.973371
188.995114	112.426134	19.205568	-0.034430	0.962441
188.698098	105.018668	19.210573	-0.034369	0.951430
188.257366	97.642631	19.215578	-0.034282	0.940300
187.835475	90.280111	19.220583	-0.034199	0.929062
187.348843	82.952942	19.225587	-0.034103	0.917723
186.549736	75.664998	19.230592	-0.033950	0.906217
186.167426	68.333983	19.235597	-0.033873	0.894611
185.785352	61.253509	19.240602	-0.033798	0.883252