Fri Mar 12 12:57:38 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.703165	-0.130229	0.000000	-0.000140	0.719265

0.232794	-0.047152	0.005005	-0.000052	0.719263
0.498942	-0.090221	0.010010	-0.000101	0.719272
0.246639	-0.056032	0.015014	-0.000054	0.719250
-0.511216	-0.066708	0.020019	0.000087	0.718963
-0.255769	-0.114480	0.025024	0.000040	0.718958
0.299345	-0.216256	0.030029	-0.000064	0.718952
0.216583	-0.198057	0.035034	-0.000048	0.718958
-0.144402	-0.137109	0.040038	0.000019	0.718952
0.530171	-0.253121	0.045043	-0.000106	0.718959
0.576601	-0.263627	0.050048	-0.000115	0.718955
0.066281	-0.173195	0.055053	-0.000019	0.718954
0.405340	-0.230598	0.060058	-0.000082	0.718959
0.603862	-0.268469	0.065062	-0.000119	0.718954
0.154556	-0.189655	0.070067	-0.000035	0.718951
-0.113087	-0.301058	0.075072	0.000015	0.718637
0.197358	-0.356926	0.080077	-0.000043	0.718636
-0.008776	-0.314461	0.085082	-0.000005	0.718647
-0.582830	-0.218369	0.090086	0.000102	0.718634
0.065463	-0.330653	0.095091	-0.000018	0.718640
0.260242	-0.365564	0.100096	-0.000054	0.718640
-0.086300	-0.361939	0.105101	0.000011	0.718525
0.153786	-0.490927	0.110106	-0.000034	0.718354
0.327287	-0.526553	0.115110	-0.000066	0.718345
-0.141937	-0.438971	0.120115	0.000021	0.718352
-0.107668	-0.447310	0.125120	0.000015	0.718348
0.459951	-0.624024	0.130125	-0.000090	0.718198
0.112109	-0.653393	0.135130	-0.000025	0.718017
-0.594992	-0.533238	0.140134	0.000106	0.718005
-0.149948	-0.608499	0.145139	0.000024	0.718013
0.510006	-0.755929	0.150144	-0.000099	0.717954
-0.518581	-0.701644	0.155149	0.000093	0.717699
-0.744899	-0.657841	0.160154	0.000135	0.717705
0.006221	-0.795835	0.165158	-0.000005	0.717697
0.162256	-0.865421	0.170163	-0.000034	0.717614
-0.567467	-0.854201	0.175168	0.000102	0.717379
-0.560072	-0.858144	0.180173	0.000101	0.717373
-0.213443	-0.915250	0.185178	0.000037	0.717382
-1.131191	-0.846942	0.190182	0.000208	0.717194
-1.371208	-0.860036	0.195187	0.000253	0.717083
-0.557472	-1.004215	0.200192	0.000101	0.717084
-0.632253	-0.994822	0.205197	0.000115	0.717076
-0.961914	-1.077915	0.210202	0.000177	0.716795
-0.707780	-1.146470	0.215206	0.000130	0.716749
-0.574316	-1.168333	0.220211	0.000105	0.716752
-1.211874	-1.155915	0.225216	0.000224	0.716552
-0.865466	-1.271368	0.230221	0.000160	0.716445
-0.216658	-1.383731	0.235226	0.000039	0.716451
-1.078755	-1.342382	0.240230	0.000200	0.716229
-1.395420	-1.334338	0.245235	0.000259	0.716133
-0.945039	-1.414825	0.250240	0.000175	0.716132
-1.010163	-1.494044	0.255245	0.000188	0.715952
-2.447443	-1.270681	0.260250	0.000455	0.715887
-2.657223	-1.236285	0.265254	0.000494	0.715881
-1.507173	-1.501742	0.270259	0.000281	0.715760
-1.752549	-1.566044	0.275264	0.000326	0.715546
-3.041308	-1.337584	0.280269	0.000566	0.715543
-2.346430	-1.482845	0.285274	0.000437	0.715500
-1.634713	-1.748930	0.290278	0.000305	0.715224
-2.154105	-1.650638	0.295283	0.000402	0.715235
-2.253142	-1.694707	0.300288	0.000420	0.715112
-2.198210	-1.811307	0.305293	0.000410	0.714900
-2.227687	-1.801003	0.310298	0.000416	0.714910
-2.111488	-1.920034	0.315302	0.000395	0.714715
-1.873429	-2.015975	0.320307	0.000350	0.714608
-2.656811	-1.886300	0.325312	0.000496	0.714588
-3.725195	-1.854799	0.330317	0.000695	0.714272
-3.579463	-1.878425	0.335322	0.000668	0.714277
-3.628387	-1.872755	0.340326	0.000678	0.714270
-4.253722	-1.899059	0.345331	0.000794	0.713997
-4.662465	-1.839257	0.350336	0.000871	0.713970
-4.383914	-1.892087	0.355341	0.000819	0.713964
-3.919618	-2.051053	0.360346	0.000733	0.713812
-4.311930	-2.065002	0.365350	0.000806	0.713645
-4.331809	-2.059165	0.370355	0.000810	0.713649
-4.095407	-2.173218	0.375360	0.000766	0.713506
-5.237750	-2.046785	0.380365	0.000979	0.713352
-5.360932	-2.019796	0.385370	0.001002	0.713362
-5.053874	-2.115412	0.390374	0.000945	0.713281
-5.789610	-2.113370	0.395379	0.001082	0.713023
-6.427148	-2.000856	0.400384	0.001201	0.713021
-6.700571	-1.955062	0.405389	0.001252	0.713015
-5.673026	-2.196679	0.410394	0.001061	0.712898
-7.141329	-2.034868	0.415398	0.001334	0.712699
-6.687928	-2.111793	0.420403	0.001250	0.712707
-7.088883	-2.038216	0.425408	0.001325	0.712711
-7.292842	-2.057638	0.430413	0.001363	0.712599
-7.975669	-2.040984	0.435418	0.001490	0.712390
-7.614072	-2.108687	0.440422	0.001423	0.712383
-7.565381	-2.115072	0.445427	0.001414	0.712387
-8.008669	-2.036968	0.450432	0.001497	0.712385
-8.208520	-2.131721	0.455437	0.001534	0.712125
-8.313406	-2.130600	0.460442	0.001554	0.712090
-8.574362	-2.087529	0.465446	0.001602	0.712083
-8.390824	-2.117472	0.470451	0.001568	0.712088
-8.388096	-2.155970	0.475456	0.001568	0.712012
-9.266138	-2.128748	0.480461	0.001732	0.711754
-9.217393	-2.132482	0.485466	0.001723	0.711764
-9.663632	-2.057137	0.490470	0.001806	0.711755
-9.279883	-2.123423	0.495475	0.001735	0.711759
-9.315663	-2.158564	0.500480	0.001741	0.711676
-10.575998	-2.046757	0.505485	0.001976	0.711451
-9.984425	-2.147731	0.510490	0.001866	0.711460
-10.264117	-2.103429	0.515494	0.001918	0.711448
-10.844884	-1.997221	0.520499	0.002027	0.711454
-9.986303	-2.149687	0.525504	0.001867	0.711454
-10.450458	-2.180147	0.530509	0.001954	0.711228
-11.185657	-2.091988	0.535514	0.002091	0.711142
-11.042787	-2.121261	0.540518	0.002064	0.711135
-10.511576	-2.212383	0.545523	0.001965	0.711141
-11.080174	-2.111862	0.550528	0.002071	0.711140
-11.446509	-2.059705	0.555533	0.002140	0.711113
-11.436209	-2.178015	0.560538	0.002138	0.710880
-11.678773	-2.140596	0.565542	0.002183	0.710868
-12.153891	-2.054346	0.570547	0.002272	0.710871
-11.713133	-2.132519	0.575552	0.002190	0.710872
-11.567009	-2.161706	0.580557	0.002163	0.710865
-11.713776	-2.208364	0.585562	0.002190	0.710720
-13.213769	-2.038162	0.590566	0.002470	0.710525
-12.421681	-2.176015	0.595571	0.002323	0.710532
-12.639967	-2.135767	0.600576	0.002363	0.710534
-13.076794	-2.062358	0.605581	0.002445	0.710525
-12.272901	-2.200986	0.610586	0.002295	0.710534
-12.500531	-2.208895	0.615590	0.002338	0.710437
-13.735714	-2.097869	0.620595	0.002568	0.710219
-13.369190	-2.163285	0.625600	0.002500	0.710218
-13.647596	-2.117870	0.630605	0.002552	0.710210
-13.651522	-2.111800	0.635610	0.002553	0.710220
-13.567794	-2.132092	0.640614	0.002537	0.710209
-13.489132	-2.142849	0.645619	0.002523	0.710215
-13.957655	-2.219209	0.650624	0.002610	0.709895
-14.890453	-2.057794	0.655629	0.002784	0.709886
-14.688682	-2.090180	0.660634	0.002746	0.709892
-13.993183	-2.217270	0.665638	0.002617	0.709886
-14.633607	-2.102728	0.670643	0.002736	0.709886
-14.715578	-2.087164	0.675648	0.002752	0.709888
-14.380460	-2.189810	0.680653	0.002690	0.709802
-15.098968	-2.164118	0.685658	0.002824	0.709597
-15.375531	-2.119298	0.690662	0.002875	0.709588
-15.494516	-2.096630	0.695667	0.002897	0.709590
-15.283690	-2.131920	0.700672	0.002858	0.709595
-15.714154	-2.057487	0.705677	0.002939	0.709590
-15.286610	-2.129917	0.710682	0.002859	0.709597
-15.531904	-2.172376	0.715686	0.002905	0.709425
-16.618307	-2.060228	0.720691	0.003107	0.709261
-16.192951	-2.134261	0.725696	0.003028	0.709265
-16.311652	-2.117806	0.730701	0.003051	0.709255
-16.164310	-2.140263	0.735706	0.003023	0.709262
-16.520074	-2.081441	0.740710	0.003090	0.709253
-16.286282	-2.120280	0.745715	0.003046	0.709258
-16.052734	-2.235635	0.750720	0.003003	0.709110
-17.753531	-2.012971	0.755725	0.003320	0.708949
-17.184261	-2.110199	0.760730	0.003214	0.708957
-16.951349	-2.156213	0.765734	0.003171	0.708948
-17.210149	-2.106950	0.770739	0.003219	0.708954
-17.338729	-2.083079	0.775744	0.003243	0.708956
-17.337446	-2.086914	0.780749	0.003243	0.708948
-17.165260	-2.170678	0.785754	0.003211	0.708841
-18.198672	-2.089643	0.790758	0.003404	0.708635
-17.984472	-2.127098	0.795763	0.003364	0.708636
-17.926845	-2.136804	0.800768	0.003353	0.708637
-18.395548	-2.055196	0.805773	0.003441	0.708633
-17.884711	-2.141235	0.810778	0.003346	0.708642
-17.891828	-2.144039	0.815782	0.003347	0.708634
-18.079840	-2.187231	0.820787	0.003382	0.708480
-19.009711	-2.084471	0.825792	0.003556	0.708354
-18.887755	-2.109772	0.830797	0.003533	0.708346
-18.568348	-2.161578	0.835802	0.003474	0.708356
-19.262357	-2.041447	0.840806	0.003603	0.708349
-18.986252	-2.089704	0.845811	0.003552	0.708350
-18.476764	-2.179479	0.850816	0.003457	0.708352
-19.151724	-2.180748	0.855821	0.003583	0.708108
-20.021731	-2.071644	0.860826	0.003745	0.708016
-19.739208	-2.127315	0.865830	0.003693	0.708005
-19.507700	-2.164704	0.870835	0.003650	0.708012
-20.051432	-2.066253	0.875840	0.003751	0.708015
-19.927035	-2.092065	0.880845	0.003728	0.708008
-19.441046	-2.172671	0.885850	0.003638	0.708019
-20.169837	-2.160078	0.890854	0.003774	0.707784
-21.060740	-2.044540	0.895859	0.003940	0.707697
-20.334860	-2.171683	0.900864	0.003805	0.707701
-20.698436	-2.110673	0.905869	0.003872	0.707693
-20.718307	-2.103376	0.910874	0.003876	0.707700
-20.733599	-2.103082	0.915878	0.003879	0.707695
-20.558148	-2.131611	0.920883	0.003847	0.707701
-20.640763	-2.232503	0.925888	0.003862	0.707468
-21.808540	-2.072763	0.930893	0.004080	0.707371
-21.310102	-2.157658	0.935898	0.003987	0.707379
-21.343294	-2.155495	0.940902	0.003994	0.707371
-21.845841	-2.064771	0.945907	0.004087	0.707373
-21.350947	-2.151252	0.950912	0.003995	0.707376
-21.676366	-2.095523	0.955917	0.004056	0.707371
-22.209659	-2.119136	0.960922	0.004155	0.707133
-22.360155	-2.121334	0.965926	0.004184	0.707074
-22.447006	-2.104667	0.970931	0.004200	0.707076
-22.338794	-2.122808	0.975936	0.004180	0.707078
-22.664037	-2.065786	0.980941	0.004241	0.707076
-22.279872	-2.130355	0.985946	0.004169	0.707084
-22.170140	-2.153861	0.990950	0.004149	0.707076
-23.119771	-2.118559	0.995955	0.004326	0.706806
-23.345058	-2.104380	1.000960	0.004368	0.706754
-23.273161	-2.122189	1.005965	0.004355	0.706743
-23.357229	-2.103336	1.010970	0.004370	0.706751
-23.521476	-2.075593	1.015974	0.004401	0.706748
-23.253536	-2.123412	1.020979	0.004351	0.706747
-23.185075	-2.133614	1.025984	0.004339	0.706751
-23.686762	-2.136874	1.030989	0.004432	0.706565
-24.336144	-2.078979	1.035994	0.004553	0.706448
-23.997032	-2.143060	1.040998	0.004491	0.706440
-24.390052	-2.072321	1.046003	0.004564	0.706442
-24.185661	-2.106638	1.051008	0.004526	0.706446
-24.202579	-2.107758	1.056013	0.004529	0.706437
-24.227479	-2.099959	1.061018	0.004534	0.706443
-24.154627	-2.183806	1.066022	0.004521	0.706301
-24.947467	-2.132539	1.071027	0.004668	0.706119
-24.996894	-2.119593	1.076032	0.004678	0.706127
-25.331844	-2.063281	1.081037	0.004740	0.706120
-24.916095	-2.133063	1.086042	0.004663	0.706129
-24.818757	-2.152453	1.091046	0.004645	0.706124
-25.380880	-2.053898	1.096051	0.004750	0.706121
-25.127652	-2.179996	1.101056	0.004703	0.705958
-25.841147	-2.103669	1.106061	0.004836	0.705855
-26.063313	-2.060513	1.111066	0.004877	0.705862
-25.871532	-2.096155	1.116070	0.004842	0.705859
-25.793803	-2.110069	1.121075	0.004827	0.705858
-25.609461	-2.139417	1.126080	0.004793	0.705865
-25.926887	-2.088090	1.131085	0.004852	0.705854
-26.292984	-2.176649	1.136090	0.004921	0.705545
-26.681283	-2.118734	1.141094	0.004993	0.705522
-27.200236	-2.026551	1.146099	0.005090	0.705521
-26.709637	-2.111545	1.151104	0.004999	0.705525
-26.918631	-2.079970	1.156109	0.005038	0.705514
-26.980042	-2.062680	1.161114	0.005049	0.705526
-26.897257	-2.081335	1.166118	0.005034	0.705518
-27.110667	-2.155004	1.171123	0.005074	0.705293
-27.823125	-2.067872	1.176128	0.005207	0.705212
-28.080522	-2.026346	1.181133	0.005255	0.705203
-27.595426	-2.107493	1.186138	0.005165	0.705214
-27.346466	-2.155423	1.191142	0.005118	0.705206
-27.559575	-2.116868	1.196147	0.005158	0.705207
-27.511819	-2.122648	1.201152	0.005150	0.705213
-27.829998	-2.200494	1.206157	0.005209	0.704941
-28.516867	-2.103910	1.211162	0.005337	0.704889
-28.570347	-2.094976	1.216166	0.005347	0.704887
-28.582429	-2.093926	1.221171	0.005349	0.704885
-28.278831	-2.144193	1.226176	0.005293	0.704892
-28.582834	-2.094666	1.231181	0.005350	0.704883
-28.343165	-2.148223	1.236186	0.005305	0.704861
-29.038176	-2.161025	1.241190	0.005435	0.704585
-29.542413	-2.071071	1.246195	0.005529	0.704585
-29.231273	-2.123538	1.251200	0.005471	0.704591
-29.000494	-2.169038	1.256205	0.005428	0.704582
-29.088917	-2.149457	1.261210	0.005445	0.704589
-29.607645	-2.058624	1.266214	0.005542	0.704585
-29.280469	-2.180802	1.271219	0.005481	0.704456
-29.704327	-2.201249	1.276224	0.005560	0.704263
-30.232920	-2.110899	1.281229	0.005658	0.704255
-30.357701	-2.085458	1.286234	0.005682	0.704261
-30.171813	-2.119740	1.291238	0.005647	0.704258
-30.071245	-2.139198	1.296243	0.005629	0.704255
-30.267601	-2.101266	1.301248	0.005665	0.704260
-30.508873	-2.157255	1.306253	0.005711	0.704061
-31.084021	-2.106013	1.311258	0.005818	0.703957
-31.090998	-2.108502	1.316262	0.005819	0.703949
-31.005045	-2.124503	1.321267	0.005803	0.703947
-30.916945	-2.135507	1.326272	0.005787	0.703957
-31.179324	-2.094899	1.331277	0.005836	0.703944
-31.060420	-2.111821	1.336282	0.005814	0.703952
-31.055004	-2.224086	1.341286	0.005813	0.703727
-32.212992	-2.063796	1.346291	0.006029	0.703634
-32.045663	-2.091056	1.351296	0.005998	0.703639
-31.827917	-2.135118	1.356301	0.005958	0.703628
-31.703065	-2.154225	1.361306	0.005935	0.703634
-32.284829	-2.051138	1.366310	0.006043	0.703633
-32.062163	-2.090701	1.371315	0.006002	0.703633
-31.815648	-2.230780	1.376320	0.005956	0.703438
-33.095275	-2.054538	1.381325	0.006194	0.703333
-32.961871	-2.074089	1.386330	0.006170	0.703342
-32.433144	-2.169343	1.391334	0.006071	0.703339
-32.887919	-2.089630	1.396339	0.006156	0.703336
-32.852644	-2.091646	1.401344	0.006150	0.703345
-32.940405	-2.082358	1.406349	0.006166	0.703331
-32.999917	-2.196123	1.411354	0.006177	0.703080
-33.805705	-2.091774	1.416358	0.006328	0.703000
-33.878039	-2.079552	1.421363	0.006341	0.702999
-33.477128	-2.146801	1.426368	0.006267	0.703007
-33.744940	-2.103049	1.431373	0.006317	0.702999
-33.775532	-2.094366	1.436378	0.006322	0.703005
-33.243510	-2.190596	1.441382	0.006224	0.703002
-34.234414	-2.160521	1.446387	0.006408	0.702705
-34.605433	-2.099600	1.451392	0.006477	0.702695
-34.624813	-2.100837	1.456397	0.006481	0.702685
-34.254550	-2.163513	1.461402	0.006412	0.702691
-34.662203	-2.091347	1.466406	0.006488	0.702690
-34.966727	-2.038072	1.471411	0.006545	0.702688
-34.262608	-2.160662	1.476416	0.006414	0.702693
-35.068003	-2.164867	1.481421	0.006564	0.702394
-35.673349	-2.068647	1.486426	0.006677	0.702370
-35.382372	-2.121667	1.491430	0.006623	0.702368
-35.095714	-2.173185	1.496435	0.006570	0.702367
-35.492821	-2.098728	1.501440	0.006644	0.702374
-35.688014	-2.067416	1.506445	0.006681	0.702366
-35.220818	-2.146607	1.511450	0.006594	0.702374
-35.744554	-2.191082	1.516454	0.006691	0.702095
-36.409820	-2.085018	1.521459	0.006815	0.702070
-36.058297	-2.143510	1.526464	0.006750	0.702078
-36.159751	-2.129374	1.531469	0.006769	0.702070
-36.365171	-2.088788	1.536474	0.006808	0.702077
-36.298705	-2.102278	1.541478	0.006795	0.702074
-36.250334	-2.134924	1.546483	0.006786	0.702025
-37.043075	-2.129775	1.551488	0.006934	0.701749
-37.078087	-2.128063	1.556493	0.006941	0.701740
-36.929342	-2.151749	1.561498	0.006913	0.701745
-37.101345	-2.121637	1.566502	0.006945	0.701744
-37.352686	-2.079614	1.571507	0.006992	0.701738
-37.066946	-2.128076	1.576512	0.006939	0.701743
-37.109485	-2.159156	1.581517	0.006947	0.701664
-38.168042	-2.082512	1.586522	0.007145	0.701437
-37.882963	-2.133904	1.591526	0.007092	0.701435
-37.838514	-2.144547	1.596531	0.007084	0.701430
-37.924496	-2.123449	1.601536	0.007100	0.701441
-38.299507	-2.061646	1.606541	0.007170	0.701431
-38.097083	-2.094251	1.611546	0.007132	0.701437
-37.853760	-2.179487	1.616550	0.007087	0.701352
-39.149255	-2.065584	1.621555	0.007328	0.701115
-38.774870	-2.126736	1.626560	0.007259	0.701126
-38.670925	-2.150338	1.631565	0.007240	0.701115
-38.834563	-2.116089	1.636570	0.007270	0.701125
-38.657976	-2.149137	1.641574	0.007237	0.701122
-38.821554	-2.122490	1.646579	0.007268	0.701117
-38.816163	-2.179111	1.651584	0.007267	0.701004
-39.629231	-2.101751	1.656589	0.007419	0.700866
-39.409521	-2.136788	1.661594	0.007378	0.700874
-39.307698	-2.155002	1.666598	0.007359	0.700874
-39.810755	-2.068201	1.671603	0.007453	0.700868
-39.314435	-2.152372	1.676608	0.007361	0.700876
-39.313318	-2.172311	1.681613	0.007361	0.700836
-40.540312	-2.101021	1.686618	0.007589	0.700537
-40.474324	-2.112767	1.691622	0.007577	0.700537
-40.483225	-2.114663	1.696627	0.007579	0.700529
-40.151222	-2.168804	1.701632	0.007517	0.700539
-40.602226	-2.092321	1.706637	0.007601	0.700531
-40.622002	-2.086001	1.711642	0.007605	0.700536
-40.188897	-2.215768	1.716646	0.007525	0.700430
-41.584566	-2.074012	1.721651	0.007785	0.700212
-41.171458	-2.143506	1.726656	0.007708	0.700220
-41.496432	-2.090188	1.731661	0.007769	0.700211
-41.437486	-2.096138	1.736666	0.007758	0.700220
-41.230148	-2.133092	1.741670	0.007719	0.700219
-41.405770	-2.103098	1.746675	0.007752	0.700216
-41.476735	-2.153722	1.751680	0.007765	0.700088
-42.659600	-2.040432	1.756685	0.007986	0.699889
-42.034203	-2.148480	1.761690	0.007870	0.699896
-41.997189	-2.154829	1.766694	0.007863	0.699896
-42.596320	-2.051807	1.771699	0.007974	0.699888
-42.142641	-2.127578	1.776704	0.007890	0.699899
-42.137544	-2.134005	1.781709	0.007889	0.699887
-42.380996	-2.149837	1.786714	0.007935	0.699767
-43.289889	-2.071284	1.791718	0.008104	0.699597
-42.915060	-2.141609	1.796723	0.008035	0.699589
-42.638057	-2.185221	1.801728	0.007983	0.699601
-43.102555	-2.106436	1.806733	0.008070	0.699592
-42.890014	-2.142359	1.811738	0.008030	0.699596
-42.771946	-2.162818	1.816742	0.008009	0.699597
-43.728359	-2.132074	1.821747	0.008187	0.699313
-43.857854	-2.129596	1.826752	0.008211	0.699271
-44.024857	-2.102980	1.831757	0.008242	0.699264
-43.816581	-2.138567	1.836762	0.008204	0.699267
-43.973478	-2.112101	1.841766	0.008233	0.699263
-43.972952	-2.114863	1.846771	0.008233	0.699258
-43.711862	-2.157371	1.851776	0.008185	0.699266
-44.706688	-2.123084	1.856781	0.008370	0.698975
-45.041190	-2.072201	1.861786	0.008432	0.698957
-44.510327	-2.165975	1.866790	0.008334	0.698958
-44.890230	-2.100465	1.871795	0.008404	0.698953
-44.728851	-2.124078	1.876800	0.008375	0.698964
-44.758540	-2.124485	1.881805	0.008380	0.698952
-44.817700	-2.112184	1.886810	0.008391	0.698955
-45.227967	-2.183312	1.891814	0.008468	0.698661
-45.724261	-2.108789	1.896819	0.008560	0.698633
-45.268681	-2.186796	1.901824	0.008476	0.698639
-45.562324	-2.136937	1.906829	0.008531	0.698634
-45.878712	-2.079796	1.911834	0.008590	0.698635
-45.472470	-2.150424	1.916838	0.008514	0.698638
-45.676389	-2.155074	1.921843	0.008552	0.698555
-46.542475	-2.098881	1.926848	0.008714	0.698354
-46.368915	-2.133268	1.931853	0.008682	0.698347
-46.383084	-2.127496	1.936858	0.008684	0.698354
-46.357581	-2.131103	1.941862	0.008680	0.698355
-46.395322	-2.128610	1.946867	0.008687	0.698346
-46.264286	-2.147354	1.951872	0.008663	0.698355
-46.726277	-2.157717	1.956877	0.008749	0.698166
-47.439664	-2.105761	1.961882	0.008882	0.698013
-46.916980	-2.199809	1.966886	0.008785	0.698011
-47.521433	-2.093665	1.971891	0.008897	0.698007
-47.532107	-2.086945	1.976896	0.008899	0.698017
-47.137715	-2.160873	1.981901	0.008826	0.698009
-47.163817	-2.156733	1.986906	0.008831	0.698008
-47.560531	-2.209786	1.991910	0.008905	0.697756
-48.312065	-2.106314	1.996915	0.009045	0.697693
-48.007486	-2.157789	2.001920	0.008989	0.697699

-48.181343	-2.125969	2.011917	0.009021	0.697700
-48.081981	-2.144839	2.021914	0.009003	0.697697
-48.038124	-2.164443	2.031910	0.008995	0.697672
-48.987552	-2.142237	2.041907	0.009172	0.697372
-48.537029	-2.152443	2.051904	0.009089	0.697515
-48.574827	-2.115301	2.061901	0.009096	0.697576
-48.481244	-2.072108	2.071898	0.009079	0.697697
-48.152468	-2.131552	2.081894	0.009018	0.697695
-48.324366	-2.099160	2.091891	0.009050	0.697698
-48.110211	-2.137584	2.101888	0.009011	0.697697
-48.217965	-2.116748	2.111885	0.009031	0.697700
-48.232686	-2.113197	2.121882	0.009034	0.697701
-48.260066	-2.110728	2.131878	0.009039	0.697696
-48.366959	-2.079259	2.141875	0.009060	0.697720
-47.290060	-2.128108	2.151872	0.008859	0.698011
-47.233536	-2.137533	2.161869	0.008849	0.698012
-47.315945	-2.123714	2.171866	0.008865	0.698010
-47.410954	-2.105381	2.181862	0.008883	0.698012
-47.358644	-2.065006	2.191859	0.008873	0.698113
-46.168931	-2.159902	2.201856	0.008652	0.698351
-46.559807	-2.089991	2.211853	0.008725	0.698350
-46.336202	-2.130215	2.221850	0.008684	0.698349
-46.455892	-2.073625	2.231846	0.008706	0.698420
-45.673097	-2.105922	2.241843	0.008561	0.698638
-45.592768	-2.119015	2.251840	0.008546	0.698640
-45.727617	-2.093154	2.261837	0.008571	0.698643
-45.296282	-2.090340	2.271834	0.008491	0.698805
-44.762905	-2.111858	2.281830	0.008392	0.698954
-44.638654	-2.131246	2.291827	0.008370	0.698959
-44.737784	-2.112332	2.301824	0.008388	0.698961
-44.341925	-2.063409	2.311821	0.008315	0.699203
-44.073567	-2.079753	2.321818	0.008265	0.699266
-44.104013	-2.074666	2.331814	0.008271	0.699265
-43.719097	-2.073195	2.341811	0.008200	0.699407
-43.016375	-2.105481	2.351808	0.008069	0.699595
-43.119984	-2.084844	2.361805	0.008089	0.699599
-43.036883	-2.099161	2.371802	0.008074	0.699600
-42.640900	-2.034930	2.381798	0.008000	0.699873
-42.142832	-2.114354	2.391795	0.007908	0.699891
-42.197752	-2.105442	2.401792	0.007918	0.699889
-42.049145	-2.046159	2.411789	0.007891	0.700062
-41.200795	-2.120426	2.421786	0.007733	0.700218
-41.405512	-2.085418	2.431782	0.007772	0.700214
-41.347987	-2.095712	2.441779	0.007761	0.700214
-40.523285	-2.087377	2.451776	0.007608	0.700528
-40.461266	-2.096506	2.461773	0.007597	0.700532
-40.336122	-2.118204	2.471770	0.007574	0.700532
-40.401043	-2.040077	2.481766	0.007586	0.700667
-39.255838	-2.142945	2.491763	0.007373	0.700872
-39.590507	-2.083841	2.501760	0.007436	0.700870
-39.550264	-2.090012	2.511757	0.007428	0.700871
-38.968080	-2.093527	2.521754	0.007320	0.701074
-38.878328	-2.087575	2.531750	0.007304	0.701118
-38.798934	-2.101267	2.541747	0.007289	0.701118
-38.537001	-2.071410	2.551744	0.007241	0.701273
-37.727840	-2.132670	2.561741	0.007090	0.701440
-37.958313	-2.093076	2.571738	0.007134	0.701437
-38.061492	-2.066027	2.581734	0.007153	0.701454
-37.195515	-2.076880	2.591731	0.006992	0.701744
-37.272926	-2.062534	2.601728	0.007007	0.701744
-36.860066	-2.135262	2.611725	0.006930	0.701746
-36.540249	-2.071650	2.621722	0.006871	0.701989
-36.288232	-2.074161	2.631718	0.006824	0.702074
-36.058188	-2.116337	2.641715	0.006782	0.702071
-36.126687	-2.062194	2.651712	0.006795	0.702156
-35.247164	-2.111799	2.661709	0.006631	0.702372
-35.293886	-2.104239	2.671706	0.006640	0.702370
-35.430106	-2.080142	2.681702	0.006666	0.702369
-34.547999	-2.110217	2.691699	0.006502	0.702625
-34.686034	-2.050912	2.701696	0.006528	0.702695
-34.106747	-2.154237	2.711693	0.006421	0.702694
-34.582751	-2.015096	2.721690	0.006509	0.702803
-33.600203	-2.089926	2.731686	0.006327	0.703006
-33.638386	-2.083387	2.741683	0.006334	0.703005
-33.635483	-2.081504	2.751680	0.006334	0.703009
-32.794200	-2.076455	2.761677	0.006178	0.703321
-32.815211	-2.062371	2.771674	0.006182	0.703342
-32.715202	-2.080007	2.781670	0.006163	0.703342
-32.466917	-2.055317	2.791667	0.006117	0.703480
-32.048138	-2.052258	2.801664	0.006040	0.703636
-31.806726	-2.094175	2.811661	0.005995	0.703638
-31.983299	-2.049059	2.821658	0.006028	0.703665
-31.198869	-2.046427	2.831654	0.005882	0.703952
-31.115657	-2.060447	2.841651	0.005867	0.703953
-31.038866	-2.074563	2.851648	0.005853	0.703952
-30.440385	-2.063020	2.861645	0.005742	0.704190
-30.231758	-2.064318	2.871642	0.005704	0.704261
-30.119909	-2.085420	2.881638	0.005683	0.704259
-30.040126	-2.056687	2.891635	0.005668	0.704345
-29.180139	-2.086497	2.901632	0.005509	0.704593
-28.981515	-2.121712	2.911629	0.005472	0.704593
-29.398858	-2.047230	2.921626	0.005550	0.704592
-28.714687	-2.066909	2.931622	0.005423	0.704798
-28.537839	-2.051527	2.941619	0.005390	0.704892
-28.433495	-2.070089	2.951616	0.005371	0.704891
-28.264264	-2.062888	2.961613	0.005340	0.704966
-27.679326	-2.045679	2.971610	0.005231	0.705210
-27.434558	-2.089080	2.981606	0.005186	0.705210
-27.643826	-2.050259	2.991603	0.005225	0.705213
-26.834539	-2.068104	3.001600	0.005075	0.705467
-26.617667	-2.077171	3.011597	0.005035	0.705526
-26.620905	-2.075350	3.021594	0.005035	0.705527
-26.564473	-2.049170	3.031590	0.005025	0.705600
-25.808376	-2.053378	3.041587	0.004885	0.705862
-25.645835	-2.081497	3.051584	0.004855	0.705863
-25.695435	-2.071450	3.061581	0.004864	0.705865
-25.321312	-2.047977	3.071578	0.004795	0.706046
-24.970943	-2.069075	3.081574	0.004730	0.706128
-25.127137	-2.041736	3.091571	0.004759	0.706127
-24.706911	-2.060390	3.101568	0.004681	0.706239
-23.820578	-2.115687	3.111565	0.004517	0.706445
-24.055946	-2.074158	3.121562	0.004561	0.706444
-24.173166	-2.053613	3.131558	0.004583	0.706443
-23.417599	-2.057010	3.141555	0.004442	0.706706
-23.219362	-2.068884	3.151552	0.004406	0.706752
-23.205589	-2.070600	3.161549	0.004403	0.706753
-23.044988	-2.026341	3.171546	0.004374	0.706899
-22.364076	-2.057411	3.181542	0.004247	0.707080
-22.457959	-2.040442	3.191539	0.004265	0.707080
-22.161276	-2.090678	3.201536	0.004210	0.707085
-21.517166	-2.058616	3.211533	0.004091	0.707379
-21.349661	-2.089525	3.221530	0.004060	0.707376
-21.485395	-2.065526	3.231526	0.004085	0.707375
-21.285475	-2.027000	3.241523	0.004048	0.707523
-20.392676	-2.097150	3.251520	0.003882	0.707701
-20.768170	-2.029092	3.261517	0.003952	0.707703
-20.614838	-2.048591	3.271514	0.003924	0.707718
-19.837205	-2.041316	3.281510	0.003780	0.708010
-19.956419	-2.018625	3.291507	0.003802	0.708013
-19.570177	-2.087858	3.301504	0.003731	0.708011
-19.255997	-2.026655	3.311501	0.003672	0.708246
-18.797285	-2.054009	3.321498	0.003587	0.708354
-18.926509	-2.031641	3.331494	0.003612	0.708352
-18.738744	-2.045528	3.341491	0.003577	0.708391
-18.075560	-2.038462	3.351488	0.003454	0.708641
-17.928672	-2.064252	3.361485	0.003427	0.708642
-17.802499	-2.088574	3.371482	0.003403	0.708637
-17.595399	-2.024335	3.381478	0.003365	0.708839
-17.095098	-2.054171	3.391475	0.003272	0.708958
-16.985275	-2.072652	3.401472	0.003252	0.708959
-17.131681	-2.026533	3.411469	0.003280	0.708999
-16.201564	-2.058058	3.421466	0.003107	0.709267
-16.290428	-2.043627	3.431462	0.003124	0.709264
-16.172364	-2.064357	3.441459	0.003102	0.709264
-15.709722	-2.040760	3.451456	0.003016	0.709475
-15.209134	-2.068009	3.461453	0.002923	0.709599
-15.110124	-2.085890	3.471450	0.002905	0.709598
-15.164265	-2.078469	3.481446	0.002915	0.709593
-14.680670	-2.027830	3.491443	0.002826	0.709866
-14.315582	-2.078861	3.501440	0.002758	0.709893
-14.368989	-2.067703	3.511437	0.002768	0.709896
-14.081970	-2.051220	3.521434	0.002715	0.710031
-13.504827	-2.060106	3.531430	0.002608	0.710218
-13.355926	-2.086800	3.541427	0.002580	0.710217
-13.552960	-2.049927	3.551424	0.002617	0.710220
-12.649042	-2.088226	3.561421	0.002449	0.710465
-12.607699	-2.061164	3.571418	0.002442	0.710533
-12.344646	-2.107495	3.581414	0.002393	0.710533
-12.077927	-2.153971	3.591411	0.002344	0.710535
-11.632116	-2.079843	3.601408	0.002261	0.710841
-11.287357	-2.125544	3.611405	0.002197	0.710872
-11.178946	-2.145256	3.621402	0.002177	0.710871
-11.477198	-2.092852	3.631398	0.002233	0.710869
-10.559775	-2.126069	3.641395	0.002063	0.711128
-10.645918	-2.105864	3.651392	0.002079	0.711137
-10.361345	-2.155479	3.661389	0.002026	0.711139
-10.557572	-2.084678	3.671386	0.002063	0.711210
-9.821415	-2.094184	3.681382	0.001926	0.711452
-9.498097	-2.151368	3.691379	0.001866	0.711452
-9.949352	-2.070881	3.701376	0.001951	0.711452
-9.183174	-2.085417	3.711373	0.001808	0.711695
-8.917844	-2.100557	3.721370	0.001759	0.711758
-8.912798	-2.100909	3.731366	0.001758	0.711759
-8.736391	-2.070131	3.741363	0.001726	0.711882
-7.938020	-2.109775	3.751360	0.001577	0.712086
-7.906699	-2.113318	3.761357	0.001572	0.712090
-8.028298	-2.092281	3.771354	0.001595	0.712088
-7.505855	-2.059422	3.781350	0.001498	0.712338
-7.001768	-2.126253	3.791347	0.001404	0.712384
-7.317022	-2.068631	3.801344	0.001463	0.712386
-6.942779	-2.065471	3.811341	0.001394	0.712524
-6.453737	-2.059356	3.821338	0.001303	0.712710
-6.255090	-2.096323	3.831334	0.001266	0.712706
-6.387170	-2.051673	3.841331	0.001291	0.712747
-5.651961	-2.044385	3.851328	0.001155	0.713022
-6.281755	-1.931468	3.861325	0.001272	0.713023
-5.515769	-2.055068	3.871322	0.001130	0.713048
-5.955069	-1.821441	3.881318	0.001212	0.713357
-4.464059	-2.085762	3.891315	0.000935	0.713359
-5.245226	-1.929138	3.901312	0.001080	0.713393
-5.132689	-1.818599	3.911309	0.001060	0.713652
-4.182877	-1.986962	3.921306	0.000883	0.713653
-5.865127	-1.587981	3.931302	0.001196	0.713850
-3.094075	-2.021169	3.941299	0.000681	0.713970
-5.327679	-1.587282	3.951296	0.001097	0.714041
-3.338010	-1.821006	3.961293	0.000727	0.714280
-4.805287	-1.556256	3.971290	0.001000	0.714286
-3.444232	-1.635864	3.981286	0.000747	0.714609
-3.327957	-1.656071	3.991283	0.000726	0.714609
-2.993844	-1.610054	4.001280	0.000664	0.714818
-3.102042	-1.544594	4.011277	0.000684	0.714910
-3.433817	-1.395659	4.021274	0.000746	0.715087
-3.238969	-1.358209	4.031270	0.000710	0.715230
-2.927186	-1.303786	4.041267	0.000652	0.715447
-2.560992	-1.317633	4.051264	0.000584	0.715549
-2.088125	-1.275609	4.061261	0.000497	0.715799
-2.164723	-1.218831	4.071258	0.000511	0.715884
-2.029873	-1.140278	4.081254	0.000486	0.716086
-2.242443	-1.056224	4.091251	0.000526	0.716177
-1.733234	-1.009193	4.101248	0.000431	0.716449
-2.267712	-0.837342	4.111245	0.000531	0.716601
-1.658173	-0.868273	4.121242	0.000418	0.716754
-1.295371	-0.775141	4.131238	0.000351	0.717066
-1.243792	-0.719905	4.141235	0.000341	0.717192
-1.087789	-0.652673	4.151232	0.000312	0.717380
-0.959286	-0.538104	4.161229	0.000289	0.717651
-1.072650	-0.418798	4.171226	0.000310	0.717847
-1.043988	-0.331566	4.181222	0.000305	0.718028
-0.651132	-0.237840	4.191219	0.000232	0.718351
-0.373809	-0.185806	4.201216	0.000181	0.718551
0.080205	-0.174477	4.211213	0.000096	0.718732
-0.056319	-0.034066	4.221210	0.000122	0.718961
0.000000	0.127041	4.231206	0.000112	0.719298

-0.433767	0.814936	4.236211	0.000192	0.720501
0.825005	1.839875	4.241216	-0.000043	0.722956
1.971039	3.504615	4.246221	-0.000257	0.726614
2.385839	5.864733	4.251226	-0.000336	0.731350
4.028231	8.516386	4.256230	-0.000643	0.737038
6.014849	11.609865	4.261235	-0.001015	0.743642
7.760192	15.223980	4.266240	-0.001342	0.751090
10.473248	19.086318	4.271245	-0.001850	0.759249
14.722717	23.124891	4.276250	-0.002643	0.768150
16.508767	28.008322	4.281254	-0.002979	0.777692
16.965365	33.467666	4.286259	-0.003067	0.787730
17.790388	39.182061	4.291264	-0.003225	0.798210
18.366189	45.222104	4.296269	-0.003336	0.809048
18.811886	51.570952	4.301274	-0.003423	0.820236
19.574345	58.120576	4.306278	-0.003569	0.831712
20.211354	64.910224	4.311283	-0.003692	0.843397
20.876779	71.923748	4.316288	-0.003820	0.855302
21.269570	79.162758	4.321293	-0.003898	0.867333
21.777622	86.574631	4.326298	-0.003997	0.879511
22.135783	94.169018	4.331302	-0.004068	0.891771
22.547720	101.905289	4.336307	-0.004150	0.904101
23.199520	109.744273	4.341312	-0.004276	0.916489
23.922292	117.676050	4.346317	-0.004416	0.928872
24.395250	125.774747	4.351322	-0.004509	0.941278
25.572634	133.837812	4.356326	-0.004734	0.953652
28.016349	141.783987	4.361331	-0.005194	0.966019
28.415706	150.187860	4.366336	-0.005273	0.978376
28.720371	158.670063	4.371341	-0.005335	0.990666
29.736624	167.082224	4.376346	-0.005530	1.002882
30.280877	175.600438	4.381350	-0.005637	1.014983
30.720087	184.176868	4.386355	-0.005724	1.026997
31.641376	192.712091	4.391360	-0.005901	1.038930
32.137793	201.330062	4.396365	-0.005999	1.050739
32.888424	209.934987	4.401370	-0.006144	1.062457
33.479075	218.592592	4.406374	-0.006260	1.074081
34.123865	227.226381	4.411379	-0.006385	1.085560
34.601968	235.914005	4.416384	-0.006480	1.096952
35.031949	244.589632	4.421389	-0.006565	1.108200
35.600106	253.261996	4.426394	-0.006677	1.119361
36.262224	261.897497	4.431398	-0.006805	1.130386
36.986672	270.532053	4.436403	-0.006946	1.141316
37.522111	279.225706	4.441408	-0.007051	1.152174
38.119773	287.853114	4.446413	-0.007168	1.162863
38.751581	296.473368	4.451418	-0.007291	1.173453
39.015452	305.126577	4.456422	-0.007345	1.183912
39.649530	313.719633	4.461427	-0.007469	1.194283
40.274079	322.288714	4.466432	-0.007591	1.204534
40.626204	330.898507	4.471437	-0.007662	1.214692
41.298771	339.448421	4.476442	-0.007792	1.224759
41.797227	348.029952	4.481446	-0.007891	1.234746
42.307085	356.561151	4.486451	-0.007991	1.244597
42.791936	365.106632	4.491456	-0.008087	1.254383
43.245139	373.614958	4.496461	-0.008176	1.264044
43.866976	382.122671	4.501466	-0.008298	1.273663
44.137038	390.637052	4.506470	-0.008353	1.283152
44.602358	399.128334	4.511475	-0.008445	1.292581
45.300732	407.561427	4.516480	-0.008581	1.301922
45.910734	416.065371	4.521485	-0.008700	1.311255
46.494227	424.547788	4.526490	-0.008814	1.320495
46.947544	432.961636	4.531494	-0.008904	1.329574
47.380403	441.381386	4.536499	-0.008989	1.338594
47.730413	449.801991	4.541504	-0.009060	1.347540
48.358269	458.172196	4.546509	-0.009182	1.356422
48.700974	466.569764	4.551514	-0.009251	1.365225
48.945797	474.989880	4.556518	-0.009302	1.373978
49.339544	483.361125	4.561523	-0.009381	1.382651
49.885942	491.723189	4.566528	-0.009488	1.391286
50.292534	500.075240	4.571533	-0.009569	1.399835
50.692005	508.420481	4.576538	-0.009649	1.408322
51.238674	516.736043	4.581542	-0.009756	1.416754
51.422755	525.093310	4.586547	-0.009795	1.425117
51.839053	533.430911	4.591552	-0.009878	1.433450
52.230355	541.726037	4.596557	-0.009956	1.441689
52.757309	550.020232	4.601562	-0.010060	1.449902
52.952215	558.361110	4.606566	-0.010101	1.458061
53.376506	566.643540	4.611571	-0.010185	1.466154
53.767168	574.994467	4.616576	-0.010263	1.474262
54.205065	583.251782	4.621581	-0.010350	1.482245
54.835429	591.487466	4.626586	-0.010473	1.490194
55.234894	599.767779	4.631590	-0.010552	1.498106
55.504839	608.043243	4.636595	-0.010608	1.505953
55.820508	616.343493	4.641600	-0.010672	1.513789
56.308873	624.564545	4.646605	-0.010768	1.521537
56.694400	632.829232	4.651610	-0.010845	1.529271
57.128183	641.076472	4.656614	-0.010931	1.536956
57.530021	649.312395	4.661619	-0.011011	1.544588
57.828542	657.604637	4.666624	-0.011072	1.552219
57.920475	665.873740	4.671629	-0.011094	1.559761
58.426228	674.064178	4.676634	-0.011194	1.567255
58.778620	682.296156	4.681638	-0.011265	1.574729
59.328120	690.489739	4.686643	-0.011372	1.582162
59.612352	698.736186	4.691648	-0.011430	1.589568
59.940710	706.962826	4.696653	-0.011497	1.596929
60.375547	715.168326	4.701658	-0.011583	1.604253
60.844834	723.365501	4.706662	-0.011675	1.611540
61.368590	731.562918	4.711667	-0.011778	1.618803
61.745910	739.778037	4.716672	-0.011854	1.626027
62.057496	748.054894	4.721677	-0.011917	1.633265
62.385331	756.253096	4.726682	-0.011983	1.640404
62.835331	764.427278	4.731686	-0.012072	1.647508
62.812518	772.676096	4.736691	-0.012073	1.654582
63.038026	780.873320	4.741696	-0.012120	1.661614
63.280206	789.059332	4.746701	-0.012171	1.668610
63.596276	797.257204	4.751706	-0.012235	1.675597
63.872294	805.424625	4.756710	-0.012291	1.682523
64.227570	813.587802	4.761715	-0.012363	1.689428
64.864871	821.731625	4.766720	-0.012486	1.696325
65.053178	829.913716	4.771725	-0.012527	1.703168
65.126349	838.140878	4.776730	-0.012545	1.710005
65.459317	846.317233	4.781734	-0.012613	1.716806
65.696110	854.479778	4.786739	-0.012662	1.723558
65.899053	862.664476	4.791744	-0.012705	1.730296
66.091899	870.840790	4.796749	-0.012746	1.737000
66.598980	878.962418	4.801754	-0.012846	1.743674
66.791969	887.135519	4.806758	-0.012887	1.750324
66.845011	895.330622	4.811763	-0.012902	1.756949
67.238130	903.470438	4.816768	-0.012980	1.763547
67.368898	911.623711	4.821773	-0.013010	1.770098
67.607433	919.800569	4.826778	-0.013059	1.776658
68.087282	927.916937	4.831782	-0.013154	1.783175
68.485456	936.067497	4.836787	-0.013233	1.789685
68.723888	944.283219	4.841792	-0.013283	1.796203
68.926062	952.405704	4.846797	-0.013325	1.802620
69.379964	960.517026	4.851802	-0.013415	1.809036
69.623492	968.671492	4.856806	-0.013466	1.815437
69.730335	976.820862	4.861811	-0.013491	1.821796
70.323647	984.921867	4.866816	-0.013606	1.828153
70.736158	993.051163	4.871821	-0.013688	1.834488
70.946163	1001.187742	4.876826	-0.013733	1.840782
71.032517	1009.352641	4.881830	-0.013754	1.847063
71.270806	1017.504989	4.886835	-0.013803	1.853330
71.716620	1025.625122	4.891840	-0.013891	1.859576
71.769129	1033.779850	4.896845	-0.013906	1.865781
72.253413	1041.921464	4.901850	-0.014002	1.872006
72.646773	1050.031832	4.906854	-0.014080	1.878176
72.700812	1058.173981	4.911859	-0.014095	1.884310
73.133742	1066.279692	4.916864	-0.014181	1.890441
73.477279	1074.403333	4.921869	-0.014250	1.896555
73.960970	1082.504569	4.926874	-0.014345	1.902648
74.234143	1090.641818	4.931878	-0.014401	1.908724
74.423354	1098.794748	4.936883	-0.014442	1.914784
74.636851	1106.921532	4.941888	-0.014487	1.920808
74.815189	1115.037496	4.946893	-0.014525	1.926801
75.188129	1123.166196	4.951898	-0.014600	1.932806
75.442253	1131.292881	4.956902	-0.014652	1.938778
75.575322	1139.406459	4.961907	-0.014682	1.944708
76.357451	1147.494597	4.966912	-0.014833	1.950673
76.533463	1155.646427	4.971917	-0.014871	1.956600
76.947147	1163.719184	4.976922	-0.014953	1.962478
77.060445	1171.845158	4.981926	-0.014979	1.968343
77.414080	1179.948495	4.986931	-0.015050	1.974201
77.791626	1188.042962	4.991936	-0.015126	1.980038
77.895041	1196.165040	4.996941	-0.015150	1.985848
78.287874	1204.272571	5.001946	-0.015228	1.991661
78.612458	1212.377055	5.006950	-0.015294	1.997448
78.987111	1220.439371	5.011955	-0.015369	2.003193
79.387474	1228.547490	5.016960	-0.015448	2.008957
79.592370	1236.682175	5.021965	-0.015492	2.014703
79.786157	1244.798470	5.026970	-0.015533	2.020418
79.988429	1252.911873	5.031974	-0.015576	2.026115
80.474448	1261.004689	5.036979	-0.015671	2.031812
80.812518	1269.116568	5.041984	-0.015740	2.037491
81.039058	1277.197697	5.046989	-0.015787	2.043121
81.354609	1285.298868	5.051994	-0.015851	2.048758
81.763027	1293.399722	5.056998	-0.015932	2.054389
81.770968	1301.518398	5.062003	-0.015939	2.059977
82.133678	1309.602036	5.067008	-0.016011	2.065560
82.595179	1317.682695	5.072013	-0.016102	2.071137
83.002569	1325.775999	5.077018	-0.016183	2.076702
83.239215	1333.875799	5.082022	-0.016232	2.082239
83.475838	1341.959838	5.087027	-0.016282	2.087751
83.939906	1350.053650	5.092032	-0.016373	2.093277
84.264706	1358.150774	5.097037	-0.016439	2.098777
84.598849	1366.231853	5.102042	-0.016506	2.104252
84.924418	1374.348758	5.107046	-0.016572	2.109737
85.046571	1382.521330	5.112051	-0.016600	2.115225
85.314524	1390.593178	5.117056	-0.016655	2.120645
85.757368	1398.616862	5.122061	-0.016742	2.126036
86.081110	1406.724469	5.127066	-0.016808	2.131458
86.241069	1414.838567	5.132070	-0.016843	2.136855
86.531607	1422.902134	5.137075	-0.016902	2.142217
87.180803	1430.957498	5.142080	-0.017028	2.147594
87.373782	1439.067002	5.147085	-0.017069	2.152950
87.520753	1447.170109	5.152090	-0.017102	2.158284
87.889218	1455.246756	5.157094	-0.017175	2.163609
88.084778	1463.316791	5.162099	-0.017217	2.168900
88.589058	1471.404014	5.167104	-0.017316	2.174217
89.139756	1479.449784	5.172109	-0.017423	2.179499
89.290294	1487.553471	5.177114	-0.017457	2.184769
89.661347	1495.650438	5.182118	-0.017531	2.190042
90.101177	1503.738347	5.187123	-0.017618	2.195303
90.381916	1511.822598	5.192128	-0.017675	2.200534
90.555745	1519.894435	5.197133	-0.017713	2.205735
90.880778	1527.980986	5.202138	-0.017778	2.210946
91.306116	1536.047577	5.207142	-0.017863	2.216142
91.633196	1544.109004	5.212147	-0.017929	2.221313
92.021003	1552.200346	5.217152	-0.018006	2.226497
92.339513	1560.279193	5.222157	-0.018071	2.231654
92.589586	1568.384573	5.227162	-0.018122	2.236810
92.910398	1576.444064	5.232166	-0.018187	2.241932
93.193321	1584.507188	5.237171	-0.018245	2.247041
93.714582	1592.598647	5.242176	-0.018347	2.252176
93.816360	1600.696109	5.247181	-0.018371	2.257267
94.024652	1608.773931	5.252186	-0.018415	2.262344
94.241454	1616.871377	5.257190	-0.018461	2.267422
94.519558	1624.999455	5.262195	-0.018517	2.272513
94.762895	1633.086963	5.267200	-0.018568	2.277564
95.072830	1641.102834	5.272205	-0.018631	2.282566
95.579276	1649.127069	5.277210	-0.018730	2.287578
95.755885	1657.225832	5.282214	-0.018768	2.292597
95.905515	1665.289669	5.287219	-0.018801	2.297582
96.596829	1673.313741	5.292224	-0.018935	2.302577
96.884900	1681.375147	5.297229	-0.018994	2.307550
97.081949	1689.491112	5.302234	-0.019035	2.312538
97.541016	1697.535730	5.307238	-0.019126	2.317493
97.594940	1705.613517	5.312243	-0.019141	2.322424
97.946976	1713.696617	5.317248	-0.019212	2.327373
98.274728	1721.771664	5.322253	-0.019278	2.332304
98.619398	1729.844717	5.327258	-0.019347	2.337225
98.856925	1737.915730	5.332262	-0.019397	2.342125
99.145369	1745.978789	5.337267	-0.019455	2.347015
99.505672	1754.080275	5.342272	-0.019528	2.351923
99.665080	1762.162920	5.347277	-0.019563	2.356794
99.967650	1770.196434	5.352282	-0.019624	2.361636
100.394260	1778.253163	5.357286	-0.019709	2.366492
100.688708	1786.292728	5.362291	-0.019768	2.371318
100.955440	1794.398743	5.367296	-0.019823	2.376170
101.325873	1802.409086	5.372301	-0.019897	2.380965
101.845040	1810.459063	5.377306	-0.019999	2.385785
101.997119	1818.584567	5.382310	-0.020033	2.390610
102.253184	1826.641608	5.387315	-0.020085	2.395394
102.528840	1834.713114	5.392320	-0.020142	2.400178
102.918781	1842.739251	5.397325	-0.020219	2.404935
103.221154	1850.810479	5.402330	-0.020281	2.409702
103.447738	1858.905304	5.407334	-0.020328	2.414467
104.007438	1866.912827	5.412339	-0.020437	2.419198
104.368583	1874.983029	5.417344	-0.020510	2.423941
104.518696	1883.073615	5.422349	-0.020543	2.428670
104.928773	1891.209378	5.427354	-0.020624	2.433436
105.258400	1899.261675	5.432358	-0.020691	2.438137
105.353517	1907.301320	5.437363	-0.020714	2.442805
105.877934	1915.325619	5.442368	-0.020816	2.447487
106.071437	1923.390139	5.447373	-0.020858	2.452159
106.345719	1931.459310	5.452378	-0.020914	2.456830
106.737300	1939.499878	5.457382	-0.020992	2.461485
107.024264	1947.546196	5.462387	-0.021050	2.466126
107.357778	1955.629328	5.467392	-0.021118	2.470783
107.573669	1963.704473	5.472397	-0.021163	2.475418
108.017638	1971.706380	5.477402	-0.021251	2.480020
108.317441	1979.768767	5.482406	-0.021312	2.484636
108.339138	1987.860725	5.487411	-0.021321	2.489240
108.746709	1995.934217	5.492416	-0.021402	2.493854
109.257593	2003.942013	5.497421	-0.021502	2.498429
109.708724	2011.989662	5.502426	-0.021591	2.503014
109.898080	2020.088329	5.507430	-0.021631	2.507600
110.064084	2028.166975	5.512435	-0.021667	2.512165
110.562090	2036.231636	5.517440	-0.021765	2.516738
110.818665	2044.255182	5.522445	-0.021818	2.521262
111.345198	2052.284911	5.527450	-0.021921	2.525800
111.484112	2060.367572	5.532454	-0.021952	2.530332
111.760844	2068.434902	5.537459	-0.022009	2.534857
112.113203	2076.474390	5.542464	-0.022080	2.539364
112.631362	2084.497721	5.547469	-0.022181	2.543866
112.904395	2092.566489	5.552474	-0.022237	2.548367
113.218442	2100.657454	5.557478	-0.022301	2.552876
113.578235	2108.691360	5.562483	-0.022373	2.557348
113.898082	2116.743767	5.567488	-0.022438	2.561820
114.009085	2124.797476	5.572493	-0.022463	2.566270
114.449610	2132.857135	5.577498	-0.022550	2.570739
114.911361	2140.915062	5.582502	-0.022642	2.575200
115.044712	2148.951694	5.587507	-0.022671	2.579619
115.419899	2157.010891	5.592512	-0.022746	2.584059
115.897621	2165.047328	5.597517	-0.022840	2.588487
116.313580	2173.233777	5.602522	-0.022923	2.592984
116.598254	2181.311207	5.607526	-0.022981	2.597405
116.845236	2189.292698	5.612531	-0.023032	2.601764
117.401501	2197.323687	5.617536	-0.023141	2.606163
117.506607	2205.349811	5.622541	-0.023166	2.610521
117.989530	2213.391836	5.627546	-0.023261	2.614907
118.449264	2221.419888	5.632550	-0.023351	2.619276
118.514501	2229.472838	5.637555	-0.023369	2.623624
118.813724	2237.527086	5.642560	-0.023429	2.627982
119.031462	2245.604079	5.647565	-0.023475	2.632339
119.335943	2253.643733	5.652570	-0.023537	2.636674
119.565651	2261.691726	5.657574	-0.023585	2.641002
119.708265	2269.727850	5.662579	-0.023616	2.645311
120.243545	2277.751223	5.667584	-0.023721	2.649631
120.403570	2285.846580	5.672589	-0.023756	2.653959
120.725815	2293.878191	5.677594	-0.023821	2.658255
121.327574	2301.878873	5.682598	-0.023938	2.662547
121.446920	2309.942212	5.687603	-0.023966	2.666833
121.658125	2318.052244	5.692608	-0.024010	2.671144
121.859572	2326.120577	5.697613	-0.024053	2.675424
122.187848	2334.124447	5.702618	-0.024119	2.679672
122.402970	2342.178033	5.707622	-0.024164	2.683932
122.840326	2350.196307	5.712627	-0.024251	2.688181
123.143638	2358.270463	5.717632	-0.024312	2.692443
123.270365	2366.339587	5.722637	-0.024341	2.696686
123.671299	2374.359279	5.727642	-0.024421	2.700913
124.029657	2382.406446	5.732646	-0.024492	2.705144
124.196122	2390.443382	5.737651	-0.024529	2.709352
124.511802	2398.554139	5.742656	-0.024592	2.713601
124.766277	2406.580697	5.747661	-0.024645	2.717796
124.947069	2414.611174	5.752666	-0.024684	2.721982
125.248165	2422.652428	5.757670	-0.024745	2.726174
125.735610	2430.644882	5.762675	-0.024841	2.730346
125.812691	2438.766218	5.767680	-0.024860	2.734553
126.018293	2446.792948	5.772685	-0.024904	2.738712
126.178050	2454.815024	5.777690	-0.024938	2.742860
126.742967	2462.840277	5.782694	-0.025049	2.747028
127.063436	2470.915398	5.787699	-0.025113	2.751200
127.400384	2479.035101	5.792704	-0.025181	2.755390
127.857100	2487.000933	5.797709	-0.025271	2.759502
127.877740	2495.042925	5.802714	-0.025280	2.763620
128.068189	2503.091086	5.807718	-0.025321	2.767745
128.491194	2511.114975	5.812723	-0.025405	2.771866
128.657146	2519.204989	5.817728	-0.025441	2.775999
129.026779	2527.204206	5.822733	-0.025515	2.780092
129.171252	2535.252095	5.827738	-0.025547	2.784189
129.605751	2543.300385	5.832742	-0.025633	2.788299
129.919197	2551.342163	5.837747	-0.025696	2.792391
130.370597	2559.393529	5.842752	-0.025785	2.796491
130.519043	2567.443763	5.847757	-0.025818	2.800566
131.057634	2575.415554	5.852762	-0.025923	2.804618
131.071312	2583.515509	5.857766	-0.025931	2.808699
131.477339	2591.532418	5.862771	-0.026012	2.812754
131.932149	2599.593475	5.867776	-0.026102	2.816829
132.129300	2607.639318	5.872781	-0.026143	2.820875
132.386507	2615.656263	5.877786	-0.026196	2.824904
132.811827	2623.707454	5.882790	-0.026281	2.828954
133.037921	2631.781267	5.887795	-0.026328	2.832999
133.147013	2639.858771	5.892800	-0.026353	2.837032
133.667017	2647.845274	5.897805	-0.026455	2.841038
133.917278	2655.867046	5.902810	-0.026507	2.845040
134.184112	2663.914112	5.907814	-0.026562	2.849051
134.421079	2671.972898	5.912819	-0.026611	2.853059
134.848035	2680.020442	5.917824	-0.026696	2.857067
135.006188	2688.070647	5.922829	-0.026730	2.861056
135.172103	2696.077517	5.927834	-0.026766	2.865018
135.471305	2704.143333	5.932838	-0.026827	2.869011
135.743651	2712.198819	5.937843	-0.026883	2.872992
136.232775	2720.231838	5.942848	-0.026979	2.876968
136.936601	2728.221708	5.947853	-0.027115	2.880929
137.346939	2736.215556	5.952858	-0.027196	2.884871
137.847807	2744.287699	5.957862	-0.027295	2.888850
138.089728	2752.341886	5.962867	-0.027345	2.892801
138.620957	2760.384720	5.967872	-0.027449	2.896757
138.798475	2768.456235	5.972877	-0.027487	2.900702
139.195972	2776.440090	5.977882	-0.027566	2.904610
139.616231	2784.518504	5.982886	-0.027650	2.908561
139.864075	2792.624559	5.987891	-0.027701	2.912510
140.214586	2800.713072	5.992896	-0.027771	2.916451
140.449951	2808.686661	5.997901	-0.027820	2.920325
140.728223	2816.684354	6.002906	-0.027877	2.924208
141.032170	2824.726895	6.007910	-0.027939	2.928108
141.038687	2832.788194	6.012915	-0.027945	2.931996
141.424660	2840.827276	6.017920	-0.028022	2.935889
141.760747	2848.830063	6.022925	-0.028090	2.939756
141.953116	2856.861135	6.027930	-0.028131	2.943624
142.187934	2864.912603	6.032934	-0.028179	2.947499
142.593946	2872.956273	6.037939	-0.028260	2.951374
142.760426	2881.041183	6.042944	-0.028296	2.955251
143.108556	2889.027657	6.047949	-0.028366	2.959086
143.541236	2897.056821	6.052954	-0.028452	2.962940
143.898433	2905.094953	6.057958	-0.028523	2.966789
144.066577	2913.131182	6.062963	-0.028560	2.970623
144.314852	2921.207425	6.067968	-0.028611	2.974475
144.598280	2929.240511	6.072973	-0.028669	2.978303
144.946083	2937.230443	6.077978	-0.028739	2.982109
145.570537	2945.266632	6.082982	-0.028860	2.985946
145.959580	2953.274435	6.087987	-0.028938	2.989753
146.145698	2961.403471	6.092992	-0.028978	2.993602
146.265130	2969.423642	6.097997	-0.029005	2.997391
146.667290	2977.426142	6.103002	-0.029085	3.001181
147.157911	2985.435620	6.108006	-0.029181	3.004974
147.305133	2993.476346	6.113011	-0.029214	3.008760
147.837645	3001.519409	6.118016	-0.029318	3.012561
147.827298	3009.619863	6.123021	-0.029321	3.016357
148.005559	3017.617352	6.128026	-0.029359	3.020110
148.702603	3025.628800	6.133030	-0.029494	3.023890
148.717249	3033.680347	6.138035	-0.029502	3.027650
149.207102	3041.744688	6.143040	-0.029598	3.031435
149.400976	3049.791110	6.148045	-0.029640	3.035192
149.588482	3057.793207	6.153050	-0.029680	3.038924
149.713989	3065.855364	6.158054	-0.029708	3.042676
149.939345	3073.881548	6.163059	-0.029755	3.046411
150.286693	3081.889624	6.168064	-0.029825	3.050140
150.483921	3089.965651	6.173069	-0.029867	3.053888
150.683548	3097.985248	6.178074	-0.029909	3.057605
150.876650	3106.039061	6.183078	-0.029950	3.061333
151.293190	3114.016259	6.188083	-0.030033	3.065032
151.482683	3122.079406	6.193088	-0.030073	3.068756
151.593772	3130.196429	6.198093	-0.030099	3.072495
151.817128	3138.258957	6.203098	-0.030146	3.076211
152.278123	3146.211250	6.208102	-0.030237	3.079882
152.457389	3154.220916	6.213107	-0.030275	3.083563
152.583902	3162.268783	6.218112	-0.030304	3.087254
152.984685	3170.297970	6.223117	-0.030383	3.090944
153.397939	3178.297410	6.228122	-0.030465	3.094617
153.893492	3186.323626	6.233126	-0.030563	3.098302
154.274296	3194.349927	6.238131	-0.030639	3.101977
154.548604	3202.398678	6.243136	-0.030695	3.105652
154.555199	3210.448842	6.248141	-0.030701	3.109312
154.765680	3218.499845	6.253146	-0.030746	3.112978
155.287780	3226.542491	6.258150	-0.030848	3.116649
155.471253	3234.540295	6.263155	-0.030887	3.120280
155.571640	3242.575090	6.268160	-0.030911	3.123920
156.237422	3250.592348	6.273165	-0.031040	3.127573
156.557101	3258.634849	6.278170	-0.031105	3.131218
156.938442	3266.691199	6.283174	-0.031181	3.134867
157.072136	3274.719784	6.288179	-0.031211	3.138488
157.486098	3282.714898	6.293184	-0.031293	3.142103
157.661034	3290.767904	6.298189	-0.031330	3.145729
157.944001	3298.790488	6.303194	-0.031388	3.149342
158.404986	3306.883792	6.308198	-0.031479	3.152990
158.586533	3314.896738	6.313203	-0.031518	3.156585
158.795876	3322.902243	6.318208	-0.031562	3.160175
158.859867	3330.946458	6.323213	-0.031579	3.163771
159.311059	3338.933643	6.328218	-0.031668	3.167354
159.601989	3347.016392	6.333222	-0.031728	3.170969
159.855031	3355.029375	6.338227	-0.031780	3.174548
160.242312	3363.080049	6.343232	-0.031857	3.178144
160.331997	3371.118714	6.348237	-0.031879	3.181718
160.734472	3379.109713	6.353242	-0.031959	3.185281
161.170838	3387.163714	6.358246	-0.032045	3.188869
161.236324	3395.222217	6.363251	-0.032062	3.192439
161.458714	3403.295308	6.368256	-0.032109	3.196018
161.833038	3411.275414	6.373261	-0.032184	3.199558
162.066947	3419.275757	6.378266	-0.032232	3.203098
162.322085	3427.337640	6.383270	-0.032285	3.206661
162.422686	3435.367175	6.388275	-0.032309	3.210200
162.720752	3443.409728	6.393280	-0.032369	3.213749
162.797655	3451.447301	6.398285	-0.032389	3.217282
162.996781	3459.460200	6.403290	-0.032431	3.220806
163.516757	3467.451179	6.408294	-0.032533	3.224329
163.703879	3475.488016	6.413299	-0.032573	3.227855
164.142994	3483.553784	6.418304	-0.032660	3.231400
164.417972	3491.631771	6.423309	-0.032716	3.234940
164.505476	3499.612330	6.428314	-0.032737	3.238426
165.011978	3507.627873	6.433318	-0.032837	3.241940
164.993601	3515.657208	6.438323	-0.032838	3.245435
165.295409	3523.670635	6.443328	-0.032900	3.248932
165.600813	3531.719843	6.448333	-0.032962	3.252442
165.819998	3539.757762	6.453338	-0.033008	3.255938
165.998639	3547.781497	6.458342	-0.033046	3.259424
166.324611	3555.788875	6.463347	-0.033112	3.262904
166.455651	3563.853118	6.468352	-0.033141	3.266398
166.872083	3571.853764	6.473357	-0.033224	3.269871
167.074766	3579.898506	6.478362	-0.033267	3.273352
167.235471	3587.971666	6.483366	-0.033302	3.276839
167.414505	3595.965551	6.488371	-0.033340	3.280289
167.772330	3603.981536	6.493376	-0.033412	3.283752
167.880301	3612.016361	6.498381	-0.033437	3.287210
167.915250	3620.056823	6.503386	-0.033449	3.290663
168.492783	3628.081756	6.508390	-0.033561	3.294127
168.553710	3636.118006	6.513395	-0.033578	3.297573
168.718547	3644.151939	6.518400	-0.033613	3.301018
168.782706	3652.170463	6.523405	-0.033630	3.304448
168.990188	3660.176545	6.528410	-0.033674	3.307876
169.227775	3668.271088	6.533414	-0.033724	3.311338
169.603368	3676.289430	6.538419	-0.033799	3.314770
169.917840	3684.281328	6.543424	-0.033862	3.318185
170.034385	3692.325534	6.548429	-0.033889	3.321610
170.242777	3700.295762	6.553434	-0.033933	3.325005
170.555567	3708.334237	6.558438	-0.033996	3.328428
170.621202	3716.406511	6.563443	-0.034014	3.331853
171.026259	3724.427186	6.568448	-0.034094	3.335266
171.364303	3732.447364	6.573453	-0.034162	3.338672
171.603377	3740.469007	6.578458	-0.034212	3.342071
171.943006	3748.500552	6.583462	-0.034280	3.345475
172.079788	3756.529904	6.588467	-0.034311	3.348867
172.396057	3764.554900	6.593472	-0.034375	3.352261
172.692187	3772.622570	6.598477	-0.034435	3.355668
172.781341	3780.640663	6.603482	-0.034456	3.359043
173.188732	3788.683377	6.608486	-0.034537	3.362437
173.444064	3796.674523	6.613491	-0.034590	3.365800
173.708737	3804.713965	6.618496	-0.034644	3.369180
173.961676	3812.767836	6.623501	-0.034697	3.372562
174.129656	3820.794606	6.628506	-0.034733	3.375927
174.332148	3828.807855	6.633510	-0.034776	3.379283
174.428337	3836.844173	6.638515	-0.034799	3.382643
174.691151	3844.868444	6.643520	-0.034853	3.386000
175.079475	3852.890965	6.648525	-0.034930	3.389357
175.056932	3860.972736	6.653530	-0.034931	3.392721
175.425729	3869.042412	6.658534	-0.035005	3.396090
175.694537	3876.978318	6.663539	-0.035060	3.399397
175.809897	3884.983075	6.668544	-0.035087	3.402723
176.006064	3892.995762	6.673549	-0.035128	3.406053
176.261533	3901.000144	6.678554	-0.035181	3.409378
176.576882	3909.067114	6.683558	-0.035245	3.412728
176.505055	3917.116830	6.688563	-0.035236	3.416053
177.001668	3925.079739	6.693568	-0.035334	3.419360
177.236562	3933.113050	6.698573	-0.035383	3.422683
177.235973	3941.142594	6.703578	-0.035388	3.425993
177.392172	3949.211786	6.708582	-0.035422	3.429322
177.761160	3957.212266	6.713587	-0.035496	3.432626
177.916968	3965.303394	6.718592	-0.035530	3.435957
178.096176	3973.292543	6.723597	-0.035568	3.439244
178.282596	3981.290360	6.728602	-0.035608	3.442532
178.737310	3989.319120	6.733606	-0.035698	3.445837
178.815907	3997.344285	6.738611	-0.035717	3.449126
179.165164	4005.401883	6.743616	-0.035788	3.452434
179.297593	4013.455030	6.748621	-0.035817	3.455729
179.380583	4021.456409	6.753626	-0.035838	3.458999
179.712356	4029.482991	6.758630	-0.035905	3.462284
179.990569	4037.490214	6.763635	-0.035962	3.465556
180.137193	4045.533278	6.768640	-0.035994	3.468836
180.397321	4053.602645	6.773645	-0.036048	3.472126
180.491280	4061.609965	6.778650	-0.036070	3.475383
180.823699	4069.620591	6.783654	-0.036137	3.478646
181.205678	4077.618044	6.788659	-0.036213	3.481902
181.387814	4085.601134	6.793664	-0.036252	3.485142
181.814778	4093.646580	6.798669	-0.036337	3.488413
182.070105	4101.673074	6.803674	-0.036390	3.491667
182.305848	4109.752000	6.808678	-0.036439	3.494939
182.690887	4117.751146	6.813683	-0.036515	3.498181
182.833824	4125.765884	6.818688	-0.036547	3.501417
182.943285	4133.786832	6.823693	-0.036572	3.504653
183.216911	4141.813407	6.828698	-0.036629	3.507893
183.631332	4149.842102	6.833702	-0.036711	3.511134
183.829674	4157.873288	6.838707	-0.036753	3.514368
184.145855	4165.889691	6.843712	-0.036817	3.517595
184.517187	4173.920287	6.848717	-0.036891	3.520828
184.624346	4181.910031	6.853722	-0.036916	3.524032
184.936347	4189.990577	6.858726	-0.036979	3.527277
185.179534	4197.997261	6.863731	-0.037030	3.530486
185.580886	4206.043911	6.868736	-0.037109	3.533714
185.548330	4214.112150	6.873741	-0.037108	3.536934
185.581474	4222.110733	6.878746	-0.037120	3.540125
185.942495	4230.138128	6.883750	-0.037192	3.543335
186.157733	4238.169794	6.888755	-0.037237	3.546539
186.288363	4246.182967	6.893760	-0.037267	3.549730
186.537056	4254.300705	6.898765	-0.037318	3.552964
186.838338	4262.315058	6.903770	-0.037379	3.556155
187.083974	4270.262150	6.908774	-0.037430	3.559315
187.160747	4278.277002	6.913779	-0.037449	3.562494
187.306012	4286.289262	6.918784	-0.037481	3.565670
187.481457	4294.338885	6.923789	-0.037519	3.568860
187.553531	4302.352821	6.928794	-0.037538	3.572030
187.819104	4310.378713	6.933798	-0.037592	3.575207
187.964633	4318.386609	6.938803	-0.037624	3.578371
188.152431	4326.402544	6.943808	-0.037665	3.581537
188.426595	4334.409867	6.948813	-0.037721	3.584698
188.622797	4342.438774	6.953818	-0.037762	3.587863
188.798138	4350.488292	6.958822	-0.037800	3.591033
188.993563	4358.506985	6.963827	-0.037841	3.594188
189.169986	4366.520657	6.968832	-0.037879	3.597339
189.287506	4374.559206	6.973837	-0.037906	3.600494
189.459998	4382.528387	6.978842	-0.037944	3.603621
189.749850	4390.589556	6.983846	-0.038003	3.606784
189.891157	4398.606218	6.988851	-0.038034	3.609924
190.032890	4406.628300	6.993856	-0.038066	3.613062
190.421984	4414.699925	6.998861	-0.038143	3.616224
190.674296	4422.648323	7.003866	-0.038195	3.619331
190.862777	4430.727575	7.008870	-0.038235	3.622485
191.064382	4438.720794	7.013875	-0.038278	3.625603
191.408247	4446.747163	7.018880	-0.038347	3.628735
191.548767	4454.834995	7.023885	-0.038378	3.631883
191.686846	4462.868158	7.028890	-0.038409	3.635006
192.294542	4470.837878	7.033894	-0.038527	3.638115
192.439340	4478.886204	7.038899	-0.038559	3.641240
192.416359	4486.861173	7.043904	-0.038560	3.644328
192.694729	4494.943215	7.048909	-0.038617	3.647464
192.697505	4502.943025	7.053914	-0.038623	3.650557
192.981806	4511.007160	7.058918	-0.038681	3.653680
193.157865	4519.020181	7.063923	-0.038719	3.656778
193.509973	4526.985187	7.068928	-0.038789	3.659860
193.752962	4535.067399	7.073933	-0.038840	3.662981
193.788636	4543.069252	7.078938	-0.038851	3.666063
194.124394	4551.068985	7.083942	-0.038919	3.669149
194.254607	4559.130060	7.088947	-0.038948	3.672251
194.412673	4567.137598	7.093952	-0.038983	3.675331
194.696386	4575.163874	7.098957	-0.039041	3.678418
194.889487	4583.210399	7.103962	-0.039082	3.681508
195.029413	4591.180080	7.108966	-0.039113	3.684565
195.126208	4599.222949	7.113971	-0.039136	3.687646
195.398099	4607.225091	7.118976	-0.039192	3.690714
195.817501	4615.279059	7.123981	-0.039275	3.693802
195.880309	4623.283223	7.128986	-0.039292	3.696860
196.268008	4631.319432	7.133990	-0.039369	3.699935
196.669371	4639.347686	7.138995	-0.039449	3.703005
196.813684	4647.351140	7.144000	-0.039481	3.706057
196.989247	4655.382214	7.149005	-0.039518	3.709117
197.426783	4663.457265	7.154010	-0.039605	3.712199
197.757497	4671.528034	7.159014	-0.039672	3.715273
197.862233	4679.484415	7.164019	-0.039696	3.718296
197.928695	4687.488481	7.169024	-0.039714	3.721333
198.317635	4695.447184	7.174029	-0.039791	3.724358
198.308181	4703.505570	7.179034	-0.039795	3.727410
198.681138	4711.505808	7.184038	-0.039869	3.730445
198.747490	4719.567686	7.189043	-0.039887	3.733495
198.905851	4727.629553	7.194048	-0.039921	3.736544
199.084470	4735.603294	7.199053	-0.039959	3.739557
199.336520	4743.600476	7.204058	-0.040011	3.742579
199.427742	4751.637512	7.209062	-0.040034	3.745610
199.581644	4759.674705	7.214067	-0.040067	3.748639
199.876847	4767.708026	7.219072	-0.040127	3.751668
200.127107	4775.729990	7.224077	-0.040179	3.754689
200.111670	4783.742521	7.229082	-0.040181	3.757698
200.200040	4791.775052	7.234086	-0.040203	3.760715
200.491620	4799.761619	7.239091	-0.040262	3.763716
200.822747	4807.785618	7.244096	-0.040329	3.766730
200.910250	4815.830228	7.249101	-0.040350	3.769744
200.948090	4823.886846	7.254106	-0.040362	3.772759
201.319242	4831.908833	7.259110	-0.040437	3.775765
201.321367	4839.948814	7.264115	-0.040442	3.778768
201.679534	4847.934414	7.269120	-0.040514	3.781756
202.065341	4855.934884	7.274125	-0.040591	3.784748
202.086408	4863.989677	7.279130	-0.040600	3.787749
202.233861	4872.031590	7.284134	-0.040632	3.790747
202.373250	4880.094692	7.289139	-0.040663	3.793749
202.607350	4888.062844	7.294144	-0.040712	3.796716
202.769975	4896.077719	7.299149	-0.040747	3.799696
203.042127	4904.035287	7.304154	-0.040803	3.802655
203.254131	4912.111360	7.309158	-0.040848	3.805654
203.449833	4920.107192	7.314163	-0.040889	3.808621
203.315779	4928.147132	7.319168	-0.040869	3.811595
203.867151	4936.142501	7.324173	-0.040977	3.814565
203.644712	4944.176481	7.329178	-0.040941	3.817530
203.914646	4952.187356	7.334182	-0.040996	3.820494
204.048392	4960.204795	7.339187	-0.041026	3.823456
204.213731	4968.230091	7.344192	-0.041062	3.826419
204.551885	4976.271309	7.349197	-0.041130	3.829390
204.768843	4984.268144	7.354202	-0.041176	3.832339
205.105177	4992.286538	7.359206	-0.041243	3.835296
205.213283	5000.308885	7.364211	-0.041268	3.838247
205.384702	5008.344946	7.369216	-0.041305	3.841203
205.665993	5016.322400	7.374221	-0.041363	3.844137
205.837994	5024.390530	7.379226	-0.041400	3.847100
205.975567	5032.396152	7.384230	-0.041431	3.850037
206.507823	5040.415017	7.389235	-0.041535	3.852984
206.514921	5048.467631	7.394240	-0.041541	3.855931
206.827602	5056.484785	7.399245	-0.041605	3.858869
206.838885	5064.531600	7.404250	-0.041612	3.861809
207.097137	5072.512002	7.409254	-0.041665	3.864728
207.224918	5080.568173	7.414259	-0.041694	3.867669
207.234624	5088.582987	7.419264	-0.041701	3.870591
207.683514	5096.823570	7.424269	-0.041790	3.873602
207.890780	5104.801505	7.429274	-0.041833	3.876510
207.929781	5112.694970	7.434278	-0.041846	3.879381
208.222013	5120.731116	7.439283	-0.041905	3.882307
208.349168	5128.681654	7.444288	-0.041934	3.885197
208.544910	5136.714564	7.449293	-0.041975	3.888116
208.694037	5144.750043	7.454298	-0.042008	3.891033
209.028194	5152.787880	7.459302	-0.042075	3.893951
209.244971	5160.825137	7.464307	-0.042121	3.896865
209.094124	5168.790245	7.469312	-0.042098	3.899744
209.423125	5176.819039	7.474317	-0.042164	3.902653
209.511609	5184.818942	7.479322	-0.042186	3.905545
209.597797	5192.853490	7.484326	-0.042207	3.908446
210.075604	5200.867756	7.489331	-0.042301	3.911346
210.009522	5208.918777	7.494336	-0.042294	3.914247
210.249231	5216.923649	7.499341	-0.042343	3.917134
210.666510	5224.888149	7.504346	-0.042426	3.920008
210.827313	5232.922101	7.509350	-0.042461	3.922901
211.031427	5240.943350	7.514355	-0.042504	3.925787
211.276931	5248.931977	7.519360	-0.042555	3.928660
211.673415	5256.995560	7.524365	-0.042634	3.931561
212.035278	5265.018233	7.529370	-0.042707	3.934444
212.137118	5273.049472	7.534374	-0.042731	3.937323
212.620964	5281.037116	7.539379	-0.042826	3.940192
212.804945	5289.039535	7.544384	-0.042865	3.943058
212.962540	5297.103324	7.549389	-0.042900	3.945944
212.982138	5305.109934	7.554394	-0.042908	3.948805
213.357789	5313.145183	7.559398	-0.042983	3.951680
213.567555	5321.209420	7.564403	-0.043027	3.954560
213.636706	5329.171686	7.569408	-0.043045	3.957399
214.030967	5337.196756	7.574413	-0.043124	3.960265
214.087745	5345.187036	7.579418	-0.043140	3.963110
214.318684	5353.194050	7.584422	-0.043188	3.965962
214.478325	5361.215611	7.589427	-0.043222	3.968816
214.688885	5369.244115	7.594432	-0.043267	3.971671
214.734543	5377.327664	7.599437	-0.043280	3.974540
214.893166	5385.318408	7.604442	-0.043315	3.977377
215.209955	5393.329528	7.609446	-0.043379	3.980222
215.459573	5401.351427	7.614451	-0.043431	3.983067
215.525667	5409.385962	7.619456	-0.043448	3.985911
215.880401	5417.390797	7.624461	-0.043519	3.988748
215.959354	5425.460188	7.629466	-0.043539	3.991601
216.134855	5433.456661	7.634470	-0.043577	3.994427
216.166669	5441.513254	7.639475	-0.043588	3.997271
216.544450	5449.467709	7.644480	-0.043663	4.000082
216.701845	5457.506183	7.649485	-0.043697	4.002917
216.605493	5465.507806	7.654490	-0.043685	4.005733
216.943924	5473.533606	7.659494	-0.043753	4.008563
217.140086	5481.569830	7.664499	-0.043794	4.011391
217.275593	5489.578085	7.669504	-0.043825	4.014207
217.602961	5497.658209	7.674509	-0.043891	4.017050
217.584008	5505.634921	7.679514	-0.043892	4.019848
217.814512	5513.646278	7.684518	-0.043940	4.022661
218.098487	5521.687739	7.689523	-0.043998	4.025483
218.194948	5529.691427	7.694528	-0.044021	4.028287
218.617840	5537.762413	7.699533	-0.044105	4.031117
218.861873	5545.872011	7.704538	-0.044156	4.033956
219.154875	5553.853032	7.709542	-0.044215	4.036749
219.341450	5561.769138	7.714547	-0.044255	4.039516
219.162217	5569.790518	7.719552	-0.044227	4.042312
219.373317	5577.795414	7.724557	-0.044271	4.045106
219.681340	5585.803632	7.729562	-0.044334	4.047901
219.799554	5593.842558	7.734566	-0.044361	4.050702
219.888008	5601.933231	7.739571	-0.044382	4.053518
220.164888	5609.902250	7.744576	-0.044439	4.056293
220.604179	5617.921335	7.749581	-0.044526	4.059086
220.771277	5625.923207	7.754586	-0.044562	4.061866
220.924835	5633.886192	7.759590	-0.044596	4.064631
221.113533	5641.982032	7.764595	-0.044636	4.067441
221.344274	5649.959261	7.769600	-0.044684	4.070209
221.464831	5658.054726	7.774605	-0.044711	4.073013
221.626407	5666.054890	7.779610	-0.044747	4.075784
221.810287	5674.045225	7.784614	-0.044786	4.078549
222.074538	5682.044179	7.789619	-0.044840	4.081317
222.190238	5689.970479	7.794624	-0.044867	4.084056
222.575810	5698.067951	7.799629	-0.044944	4.086855
222.643656	5706.088566	7.804634	-0.044961	4.089622
222.822849	5714.100313	7.809638	-0.045000	4.092385
223.145173	5722.131926	7.814643	-0.045065	4.095155
223.124218	5730.134343	7.819648	-0.045066	4.097909
223.493185	5738.177939	7.824653	-0.045140	4.100680
223.745434	5746.178005	7.829658	-0.045192	4.103433
223.766061	5754.201501	7.834662	-0.045201	4.106188
224.022771	5762.244175	7.839667	-0.045254	4.108952
224.247029	5770.232594	7.844672	-0.045301	4.111695
224.544404	5778.333952	7.849677	-0.045361	4.114475
224.537832	5786.343794	7.854682	-0.045365	4.117219
224.617765	5794.309226	7.859686	-0.045385	4.119946
224.937732	5802.340473	7.864691	-0.045450	4.122697
225.296504	5810.288082	7.869696	-0.045521	4.125418
225.459171	5818.388167	7.874701	-0.045557	4.128187
225.611742	5826.423688	7.879706	-0.045590	4.130932
225.621494	5834.440508	7.884710	-0.045597	4.133667
225.981439	5842.471999	7.889715	-0.045669	4.136409
225.910388	5850.445605	7.894720	-0.045661	4.139125
226.305079	5858.542650	7.899725	-0.045740	4.141886
226.375166	5866.484216	7.904730	-0.045758	4.144589
226.562610	5874.504018	7.909734	-0.045798	4.147318
226.814831	5882.564597	7.914739	-0.045850	4.150059
226.869670	5890.603478	7.919744	-0.045865	4.152790
227.117536	5898.613366	7.924749	-0.045916	4.155510
227.288000	5906.619311	7.929754	-0.045953	4.158227
227.433871	5914.637866	7.934758	-0.045986	4.160946
227.721009	5922.595122	7.939763	-0.046044	4.163644
227.665620	5930.637578	7.944768	-0.046039	4.166365
228.046258	5938.692724	7.949773	-0.046115	4.169094
228.222312	5946.680709	7.954778	-0.046153	4.171796
228.420341	5954.677841	7.959782	-0.046195	4.174499
228.682676	5962.782666	7.964787	-0.046249	4.177238
228.896059	5970.726960	7.969792	-0.046293	4.179920
229.137377	5978.766327	7.974797	-0.046343	4.182633
229.253887	5986.767805	7.979802	-0.046370	4.185329
229.492249	5994.783541	7.984806	-0.046420	4.188031
229.954020	6002.794581	7.989811	-0.046511	4.190731
230.152056	6010.916954	7.994816	-0.046553	4.193464
230.382481	6018.917275	7.999821	-0.046601	4.196154
230.438723	6026.877182	8.004826	-0.046616	4.198828
230.542115	6034.899343	8.009830	-0.046641	4.201521
230.690255	6042.868496	8.014835	-0.046673	4.204195
230.976835	6050.910251	8.019840	-0.046732	4.206893
231.086721	6058.880681	8.024845	-0.046757	4.209563
231.218829	6066.961913	8.029850	-0.046787	4.212269
231.603081	6074.957634	8.034854	-0.046863	4.214948
231.748661	6082.999455	8.039859	-0.046896	4.217637
231.694889	6090.969262	8.044864	-0.046891	4.220299
232.130921	6098.983722	8.049869	-0.046977	4.222979
232.143772	6107.005710	8.054874	-0.046984	4.225656
232.442549	6114.998148	8.059878	-0.047045	4.228323
232.722906	6123.081592	8.064883	-0.047103	4.231020
232.639011	6131.102121	8.069888	-0.047092	4.233690
232.753125	6139.174522	8.074893	-0.047118	4.236377
233.142340	6147.084576	8.079898	-0.047196	4.239011
233.404339	6155.120793	8.084902	-0.047250	4.241685
233.507626	6163.083002	8.089907	-0.047274	4.244330
233.757003	6171.117626	8.094912	-0.047326	4.247000
233.980027	6179.151560	8.099917	-0.047372	4.249667
234.045969	6187.214773	8.104922	-0.047390	4.252340
234.146294	6195.251986	8.109926	-0.047413	4.255004
234.470722	6203.266468	8.114931	-0.047479	4.257661
234.692025	6211.283228	8.119936	-0.047525	4.260315
234.822282	6219.294314	8.124941	-0.047554	4.262965
234.767910	6227.338061	8.129946	-0.047549	4.265623
235.143533	6235.329066	8.134950	-0.047624	4.268266
235.252526	6243.382354	8.139955	-0.047650	4.270925
235.343116	6251.364504	8.144960	-0.047672	4.273558
235.677696	6259.472237	8.149965	-0.047739	4.276234
235.970627	6267.406152	8.154970	-0.047799	4.278850
235.958125	6275.425892	8.159974	-0.047801	4.281490
236.083178	6283.479366	8.164979	-0.047830	4.284141
236.220702	6291.450198	8.169984	-0.047861	4.286764
236.474950	6299.470573	8.174989	-0.047913	4.289401
236.587623	6307.520423	8.179994	-0.047939	4.292046
236.856421	6315.522926	8.184998	-0.047994	4.294675
237.170358	6323.585521	8.190003	-0.048058	4.297322
237.246951	6331.524637	8.195008	-0.048077	4.299925
237.465671	6339.568142	8.200013	-0.048123	4.302562
237.604961	6347.558475	8.205018	-0.048154	4.305179
237.704547	6355.634844	8.210022	-0.048178	4.307822
237.789457	6363.622973	8.215027	-0.048198	4.310435
238.042137	6371.664652	8.220032	-0.048251	4.313065
238.159519	6379.679085	8.225037	-0.048277	4.315684
238.421672	6387.678869	8.230042	-0.048331	4.318297
238.628978	6395.667621	8.235046	-0.048375	4.320904
238.891428	6403.754889	8.240051	-0.048429	4.323543
238.849858	6411.673769	8.245056	-0.048426	4.326122
239.089694	6419.739821	8.250061	-0.048476	4.328750
239.348499	6427.768238	8.255066	-0.048529	4.331365
239.352365	6435.752405	8.260070	-0.048535	4.333961
239.511314	6443.837007	8.265075	-0.048570	4.336590
239.643312	6451.777174	8.270080	-0.048599	4.339170
239.904584	6459.811755	8.275085	-0.048653	4.341780
239.978288	6467.812846	8.280090	-0.048672	4.344376
240.172325	6475.849982	8.285094	-0.048713	4.346984
240.362312	6483.884401	8.290099	-0.048754	4.349588
240.424819	6491.910878	8.295104	-0.048770	4.352188
240.804377	6499.989849	8.300109	-0.048846	4.354805
241.010798	6507.984598	8.305114	-0.048890	4.357392
241.045779	6515.918975	8.310118	-0.048901	4.359957
241.253898	6523.952299	8.315123	-0.048945	4.362554
241.482198	6531.923369	8.320128	-0.048993	4.365129
241.597028	6539.971099	8.325133	-0.049019	4.367726
241.626829	6548.007852	8.330138	-0.049030	4.370318
241.944123	6556.024627	8.335142	-0.049094	4.372904
242.241479	6564.056347	8.340147	-0.049154	4.375493
242.080047	6572.044132	8.345152	-0.049129	4.378063
242.332441	6580.055248	8.350157	-0.049181	4.380642
242.715900	6588.090207	8.355162	-0.049258	4.383228
242.872187	6596.074824	8.360166	-0.049292	4.385794
243.055426	6604.113308	8.365171	-0.049331	4.388377
243.294218	6612.155643	8.370176	-0.049381	4.390959
243.395619	6620.192520	8.375181	-0.049405	4.393538
243.541564	6628.227564	8.380186	-0.049437	4.396114
243.617282	6636.139900	8.385190	-0.049456	4.398650
244.090895	6644.270656	8.390195	-0.049550	4.401256
244.064312	6652.211645	8.395200	-0.049550	4.403797
244.314313	6660.277721	8.400205	-0.049601	4.406377
244.541428	6668.235663	8.405210	-0.049649	4.408922
244.557096	6676.275944	8.410214	-0.049657	4.411491
244.841231	6684.394985	8.415219	-0.049715	4.414084
245.098220	6692.365674	8.420224	-0.049768	4.416629
245.306335	6700.332999	8.425229	-0.049811	4.419170
245.399957	6708.369437	8.430234	-0.049834	4.421732
245.463932	6716.320816	8.435238	-0.049851	4.424265
245.864382	6724.419011	8.440243	-0.049931	4.426844
245.966179	6732.402730	8.445248	-0.049955	4.429385
245.876495	6740.438008	8.450253	-0.049943	4.431939
246.102978	6748.494086	8.455258	-0.049990	4.434500
246.367129	6756.521945	8.460262	-0.050045	4.437051
246.536835	6764.489906	8.465267	-0.050081	4.439581
246.597884	6772.506283	8.470272	-0.050098	4.442124
246.813279	6780.481894	8.475277	-0.050143	4.444653
246.960512	6788.560607	8.480282	-0.050175	4.447214
247.220102	6796.506501	8.485286	-0.050229	4.449731
247.328380	6804.592136	8.490291	-0.050254	4.452290
247.391881	6812.589239	8.495296	-0.050271	4.454820
247.689124	6820.638425	8.500301	-0.050331	4.457366
247.962286	6828.606634	8.505306	-0.050387	4.459884
247.924058	6836.603945	8.510310	-0.050385	4.462409
248.055716	6844.641388	8.515315	-0.050415	4.464946
248.222294	6852.672168	8.520320	-0.050451	4.467480
248.528311	6860.692130	8.525325	-0.050513	4.470009
248.519377	6868.710358	8.530330	-0.050516	4.472535
248.597370	6876.736140	8.535334	-0.050536	4.475062
249.001051	6884.757039	8.540339	-0.050616	4.477588
249.088395	6892.738312	8.545344	-0.050638	4.480098
249.122479	6900.726642	8.550349	-0.050649	4.482609
249.261201	6908.782030	8.555354	-0.050680	4.485140
249.565509	6916.743896	8.560359	-0.050742	4.487641
249.694475	6924.809577	8.565363	-0.050771	4.490172
249.748932	6932.822827	8.570368	-0.050786	4.492685
249.932319	6940.879236	8.575373	-0.050825	4.495211
250.274460	6948.870009	8.580378	-0.050894	4.497715
250.302614	6956.831298	8.585383	-0.050904	4.500208
250.533218	6964.914998	8.590387	-0.050952	4.502738
250.663664	6972.857415	8.595392	-0.050982	4.505222
250.701980	6980.923946	8.600397	-0.050994	4.507743
251.268682	6988.955683	8.605402	-0.051105	4.510254
251.209333	6996.984147	8.610407	-0.051099	4.512760
251.314506	7005.073818	8.615411	-0.051123	4.515284
251.339830	7013.012458	8.620416	-0.051133	4.517760
251.562769	7020.981051	8.625421	-0.051180	4.520244
251.787085	7028.975165	8.630426	-0.051227	4.522735
251.781663	7036.948319	8.635431	-0.051231	4.525217
251.937029	7045.031136	8.640435	-0.051265	4.527733
252.241539	7053.040201	8.645440	-0.051326	4.530224
252.395968	7061.083911	8.650445	-0.051360	4.532725
252.550958	7069.101967	8.655450	-0.051394	4.535216
252.717510	7077.065085	8.660455	-0.051430	4.537688
252.835461	7085.104360	8.665459	-0.051457	4.540183
252.880736	7093.121336	8.670464	-0.051471	4.542669
253.176166	7101.074858	8.675469	-0.051531	4.545135
253.435331	7109.149950	8.680474	-0.051584	4.547637
253.343721	7117.151709	8.685479	-0.051572	4.550114
253.526567	7125.257370	8.690483	-0.051611	4.552623
253.603490	7133.214600	8.695488	-0.051631	4.555084
253.964075	7141.272886	8.700493	-0.051703	4.557575
254.020353	7149.245060	8.705498	-0.051719	4.560038
254.251396	7157.241079	8.710503	-0.051767	4.562508
254.480548	7165.260761	8.715507	-0.051814	4.564983
254.537305	7173.305789	8.720512	-0.051830	4.567464
254.836195	7181.288514	8.725517	-0.051891	4.569925
254.934043	7189.367565	8.730522	-0.051914	4.572414
254.978907	7197.337645	8.735527	-0.051928	4.574869
255.193461	7205.388645	8.740531	-0.051973	4.577346
255.361288	7213.339656	8.745536	-0.052009	4.579792
255.626828	7221.419684	8.750541	-0.052063	4.582276
255.694056	7229.407108	8.755546	-0.052081	4.584731
255.912677	7237.411734	8.760551	-0.052127	4.587189
256.108137	7245.483877	8.765555	-0.052168	4.589667
256.163187	7253.530176	8.770560	-0.052184	4.592135
256.542939	7261.553832	8.775565	-0.052260	4.594595
256.635707	7269.609864	8.780570	-0.052282	4.597063
256.606523	7277.470559	8.785575	-0.052281	4.599471
256.937051	7285.568633	8.790579	-0.052348	4.601950
257.121340	7293.486569	8.795584	-0.052387	4.604372
257.304050	7301.563996	8.800589	-0.052427	4.606842
257.487118	7309.569195	8.805594	-0.052466	4.609288
257.699418	7317.620639	8.810599	-0.052510	4.611748
258.017947	7325.666237	8.815603	-0.052575	4.614204
258.120018	7333.653784	8.820608	-0.052599	4.616641
258.341889	7341.605702	8.825613	-0.052645	4.619065
258.450228	7349.688883	8.830618	-0.052671	4.621529
258.468656	7357.666667	8.835623	-0.052679	4.623959
258.712667	7365.729904	8.840627	-0.052730	4.626414
258.900002	7373.683548	8.845632	-0.052769	4.628834
259.043997	7381.736870	8.850637	-0.052801	4.631283
259.082397	7389.794358	8.855642	-0.052814	4.633733
259.284607	7397.794738	8.860647	-0.052856	4.636163
259.584282	7405.785191	8.865651	-0.052917	4.638589
259.613110	7413.778352	8.870656	-0.052928	4.641015
259.761051	7421.729658	8.875661	-0.052960	4.643427
260.155891	7429.806296	8.880666	-0.053039	4.645875
260.392351	7437.818909	8.885671	-0.053088	4.648303
260.458036	7445.858004	8.890675	-0.053105	4.650737
260.444858	7453.846421	8.895680	-0.053108	4.653155
260.570501	7461.903448	8.900685	-0.053136	4.655593
260.716153	7469.917316	8.905690	-0.053169	4.658016
260.805654	7477.858748	8.910695	-0.053190	4.660415
261.053998	7485.934161	8.915699	-0.053242	4.662854
261.015699	7493.891719	8.920704	-0.053240	4.665257
261.300792	7501.954099	8.925709	-0.053298	4.667689
261.585896	7509.983524	8.930714	-0.053356	4.670110
261.514362	7518.035266	8.935719	-0.053348	4.672537
261.729020	7526.176521	8.940723	-0.053393	4.674990
261.914412	7534.086567	8.945728	-0.053432	4.677371
262.116136	7541.993543	8.950733	-0.053475	4.679750
262.070486	7550.052789	8.955738	-0.053472	4.682175
262.168833	7557.989245	8.960743	-0.053495	4.684560
262.627369	7566.101283	8.965747	-0.053585	4.686997
262.580914	7574.008815	8.970752	-0.053582	4.689372
262.693808	7582.130442	8.975757	-0.053608	4.691810
263.046506	7590.151705	8.980762	-0.053679	4.694216
263.111312	7598.120135	8.985767	-0.053696	4.696605
262.952887	7606.124486	8.990771	-0.053671	4.699004
263.252548	7614.171512	8.995776	-0.053732	4.701414
263.570672	7622.153040	9.000781	-0.053797	4.703803
263.717799	7630.209502	9.005786	-0.053829	4.706213
263.669712	7638.209171	9.010791	-0.053825	4.708606
264.052228	7646.206833	9.015795	-0.053902	4.710996
264.085700	7654.280145	9.020800	-0.053913	4.713408
264.267785	7662.274121	9.025805	-0.053952	4.715795
264.724893	7670.270331	9.030810	-0.054042	4.718180
264.766056	7678.287112	9.035815	-0.054055	4.720572
264.919126	7686.329905	9.040819	-0.054088	4.722969
264.949526	7694.292976	9.045824	-0.054099	4.725343
265.301815	7702.363649	9.050829	-0.054170	4.727746
265.415737	7710.378661	9.055834	-0.054196	4.730131
265.602159	7718.398460	9.060839	-0.054236	4.732517
265.970703	7726.435703	9.065843	-0.054310	4.734906
265.888873	7734.420170	9.070848	-0.054299	4.737280
266.057842	7742.389076	9.075853	-0.054336	4.739647
266.208780	7750.479632	9.080858	-0.054369	4.742049
266.412331	7758.388679	9.085863	-0.054412	4.744396
266.528386	7766.497642	9.090867	-0.054439	4.746801
266.597542	7774.480716	9.095872	-0.054457	4.749168
266.794807	7782.531394	9.100877	-0.054499	4.751553
267.111984	7790.626560	9.105882	-0.054563	4.753950
267.167726	7798.572108	9.110887	-0.054578	4.756302
267.336701	7806.576759	9.115891	-0.054615	4.758670
267.318354	7814.560021	9.120896	-0.054616	4.761031
267.439530	7822.538363	9.125901	-0.054644	4.763389
267.772006	7830.588826	9.130906	-0.054711	4.765767
267.888749	7838.583661	9.135911	-0.054738	4.768127
267.965780	7846.607399	9.140915	-0.054757	4.770495
268.129089	7854.636268	9.145920	-0.054793	4.772863
268.467506	7862.703245	9.150925	-0.054861	4.775241
268.529724	7870.670071	9.155930	-0.054878	4.777589
268.521354	7878.662164	9.160935	-0.054881	4.779943
268.886452	7886.718431	9.165939	-0.054954	4.782313
268.982740	7894.666898	9.170944	-0.054977	4.784652
269.095950	7902.712963	9.175949	-0.055003	4.787018
269.088625	7910.720986	9.180954	-0.055007	4.789373
269.357193	7918.759238	9.185959	-0.055062	4.791733
269.557798	7926.768676	9.190963	-0.055105	4.794085
269.597051	7934.844640	9.195968	-0.055117	4.796455
269.774607	7942.762787	9.200973	-0.055155	4.798778
269.885792	7950.833980	9.205978	-0.055181	4.801144
269.897737	7958.777707	9.210983	-0.055188	4.803473
270.164319	7966.829453	9.215987	-0.055243	4.805831
270.312791	7974.838613	9.220992	-0.055276	4.808175
270.360814	7982.856548	9.225997	-0.055290	4.810522
270.621658	7990.384422	9.231002	-0.055343	4.812723
270.696913	7995.060618	9.236007	-0.055360	4.814090

270.809947	7997.311274	9.241011	-0.055382	4.814747
270.812114	7998.669717	9.246016	-0.055383	4.815144
270.965213	7999.144260	9.251021	-0.055412	4.815282
270.977309	7999.776725	9.256026	-0.055415	4.815467
270.838640	7999.741336	9.261031	-0.055389	4.815458
271.027783	7999.767912	9.266035	-0.055424	4.815464
271.103325	7999.728548	9.271040	-0.055438	4.815453
271.049972	7999.749025	9.276045	-0.055428	4.815459
271.233300	7999.768030	9.281050	-0.055462	4.815464
271.263596	7999.706565	9.286055	-0.055467	4.815445
271.400933	7999.744044	9.291059	-0.055492	4.815456
271.346884	7999.746352	9.296064	-0.055482	4.815457
271.397483	7999.730078	9.301069	-0.055492	4.815452
271.502935	7999.738198	9.306074	-0.055511	4.815454
271.379093	7999.732956	9.311079	-0.055488	4.815453
271.600635	7999.799582	9.316083	-0.055529	4.815471
271.672367	7999.748407	9.321088	-0.055542	4.815456
271.688634	7999.765750	9.326093	-0.055545	4.815461
271.623230	7999.786029	9.331098	-0.055533	4.815467
271.660360	7999.733220	9.336103	-0.055539	4.815451
271.697315	7999.775467	9.341107	-0.055546	4.815464
271.664612	7999.726856	9.346112	-0.055540	4.815449
271.797810	7999.756792	9.351117	-0.055565	4.815458
271.877533	7999.765559	9.356122	-0.055579	4.815460
271.755626	7999.731511	9.361127	-0.055557	4.815450
271.931064	7999.751457	9.366131	-0.055589	4.815455
271.869732	7999.746169	9.371136	-0.055577	4.815454
271.821899	7999.776348	9.376141	-0.055568	4.815463
271.741619	7999.787840	9.381146	-0.055553	4.815467
271.787690	7999.747994	9.386151	-0.055562	4.815455
271.977533	7999.866439	9.391155	-0.055597	4.815489
271.960665	7999.986845	9.396160	-0.055594	4.815524
271.955951	7999.733618	9.401165	-0.055593	4.815450
272.215088	7999.784840	9.406170	-0.055641	4.815464
271.884371	7999.850980	9.411175	-0.055579	4.815485
272.089722	7999.767811	9.416179	-0.055617	4.815459
271.909303	7999.841750	9.421184	-0.055583	4.815482
272.164735	7999.769013	9.426189	-0.055631	4.815459
272.292368	7999.891783	9.431194	-0.055655	4.815495
272.065191	7999.747066	9.436199	-0.055612	4.815454
272.165093	7999.791411	9.441203	-0.055631	4.815466
272.010530	7999.843343	9.446208	-0.055602	4.815482
272.214258	7999.999401	9.451213	-0.055640	4.815527
272.289418	7999.844675	9.456218	-0.055653	4.815481
272.155607	7999.851019	9.461223	-0.055628	4.815483
272.333657	7999.768471	9.466227	-0.055661	4.815459
272.401449	7999.847539	9.471232	-0.055674	4.815481
272.337011	7999.853949	9.476237	-0.055662	4.815483
272.411898	7999.762237	9.481242	-0.055675	4.815456
272.203913	7999.935058	9.486247	-0.055637	4.815508
272.346425	7999.781435	9.491251	-0.055663	4.815462
272.560373	7999.861825	9.496256	-0.055703	4.815485
272.378386	7999.777660	9.501261	-0.055668	4.815461
272.407204	7999.764234	9.506266	-0.055674	4.815457
272.306102	7999.878990	9.511271	-0.055655	4.815491
272.483277	7999.792155	9.516275	-0.055688	4.815465
272.434085	7999.851151	9.521280	-0.055678	4.815482
272.448117	7999.750967	9.526285	-0.055681	4.815453
272.452176	7999.768111	9.531290	-0.055681	4.815458
272.557564	7999.846725	9.536295	-0.055701	4.815480
272.655160	7999.786359	9.541299	-0.055719	4.815462
272.437823	7999.846878	9.546304	-0.055678	4.815481
272.538256	7999.874143	9.551309	-0.055697	4.815488
272.684137	7999.850882	9.556314	-0.055724	4.815481
272.739111	7999.797296	9.561319	-0.055734	4.815465
272.541278	7999.823954	9.566323	-0.055697	4.815474
272.558518	7999.989780	9.571328	-0.055700	4.815522
272.667383	7999.853762	9.576333	-0.055720	4.815482
272.647703	7999.774388	9.581338	-0.055716	4.815459
272.572708	7999.855393	9.586343	-0.055702	4.815483
272.623688	7999.760085	9.591347	-0.055712	4.815455
272.729264	7999.860065	9.596352	-0.055731	4.815483
272.511686	7999.764637	9.601357	-0.055690	4.815457
272.732206	7999.763959	9.606362	-0.055731	4.815455
272.627256	7999.937399	9.611367	-0.055712	4.815507
272.620798	7999.770656	9.616371	-0.055710	4.815458
272.538636	7999.833386	9.621376	-0.055695	4.815477
272.619257	7999.869939	9.626381	-0.055710	4.815487
272.715293	7999.776437	9.631386	-0.055728	4.815459
272.699772	7999.931046	9.636391	-0.055725	4.815504
272.933677	7999.766099	9.641395	-0.055768	4.815455
272.723057	7999.756232	9.646400	-0.055729	4.815453
272.714216	7999.851136	9.651405	-0.055727	4.815481
272.958425	7999.781420	9.656410	-0.055772	4.815459
272.788043	7999.861932	9.661415	-0.055740	4.815484
272.670862	7999.794848	9.666419	-0.055718	4.815465
272.856709	7999.865167	9.671424	-0.055753	4.815484
272.814739	7999.784360	9.676429	-0.055745	4.815461
272.782280	7999.793429	9.681434	-0.055739	4.815464
272.923535	7999.856610	9.686439	-0.055765	4.815482
272.813286	7999.770413	9.691443	-0.055744	4.815457
272.909423	7999.767701	9.696448	-0.055762	4.815456
272.737016	7999.797979	9.701453	-0.055730	4.815465
272.841323	7999.781515	9.706458	-0.055749	4.815460
272.822190	7999.949951	9.711463	-0.055745	4.815509
272.762246	7999.884871	9.716467	-0.055734	4.815491
272.823781	7999.760896	9.721472	-0.055745	4.815454
272.829962	7999.860319	9.726477	-0.055746	4.815483
273.054549	7999.842619	9.731482	-0.055788	4.815477
272.903115	7999.861491	9.736487	-0.055760	4.815483
272.907675	7999.780377	9.741491	-0.055760	4.815459
273.007008	7999.874915	9.746496	-0.055779	4.815487
272.927847	7999.768932	9.751501	-0.055764	4.815456
272.913972	7999.849869	9.756506	-0.055761	4.815480
272.887486	7999.851559	9.761511	-0.055756	4.815480
272.934125	7999.851242	9.766515	-0.055764	4.815480
272.837353	7999.851782	9.771520	-0.055746	4.815481
273.036611	7999.757832	9.776525	-0.055783	4.815452
273.008893	7999.789409	9.781530	-0.055778	4.815462
272.865326	7999.910948	9.786535	-0.055751	4.815498
273.072743	7999.858788	9.791539	-0.055790	4.815482
273.041421	7999.767473	9.796544	-0.055784	4.815455
272.844326	7999.890273	9.801549	-0.055747	4.815492
272.952337	7999.848235	9.806554	-0.055767	4.815479
273.040185	7999.758871	9.811559	-0.055783	4.815453
273.004226	7999.876830	9.816563	-0.055776	4.815487
272.911746	7999.758881	9.821568	-0.055759	4.815453
272.953121	7999.967827	9.826573	-0.055766	4.815514
273.043744	7999.788786	9.831578	-0.055783	4.815461
272.901850	7999.844130	9.836583	-0.055756	4.815478
272.970554	7999.767269	9.841587	-0.055769	4.815455
273.066235	7999.872429	9.846592	-0.055787	4.815486
272.771201	7999.840887	9.851597	-0.055732	4.815478
273.038309	7999.785430	9.856602	-0.055781	4.815460
273.115341	7999.762111	9.861607	-0.055795	4.815453
273.069735	7999.867096	9.866611	-0.055787	4.815484
273.031422	7999.767122	9.871616	-0.055780	4.815455
273.087347	7999.875904	9.876621	-0.055790	4.815487
273.152325	7999.808595	9.881626	-0.055802	4.815467
273.252219	7999.772833	9.886631	-0.055820	4.815456
273.161527	7999.794835	9.891635	-0.055803	4.815463
273.146774	7999.887507	9.896640	-0.055800	4.815490
273.039903	7999.786412	9.901645	-0.055780	4.815461
273.151766	7999.789297	9.906650	-0.055801	4.815461
273.261690	7999.784675	9.911655	-0.055821	4.815459
273.151418	7999.794607	9.916659	-0.055801	4.815463
273.194604	7999.875410	9.921664	-0.055809	4.815486
273.232528	7999.775615	9.926669	-0.055815	4.815457
273.273112	7999.806174	9.931674	-0.055823	4.815465
273.083075	7999.753919	9.936679	-0.055787	4.815451
273.202355	7999.875487	9.941683	-0.055809	4.815486
273.264735	7999.801727	9.946688	-0.055821	4.815464
273.109218	7999.871801	9.951693	-0.055792	4.815485
273.163253	7999.794701	9.956698	-0.055802	4.815463
273.287267	7999.768946	9.961703	-0.055825	4.815454
273.138669	7999.785728	9.966707	-0.055797	4.815460
273.072169	7999.775015	9.971712	-0.055784	4.815457
273.248304	7999.790702	9.976717	-0.055817	4.815461
273.279024	7999.915094	9.981722	-0.055823	4.815497
273.206071	7999.779304	9.986727	-0.055809	4.815458
273.264428	7999.799473	9.991731	-0.055820	4.815464
273.326326	7999.796201	9.996736	-0.055831	4.815462
273.105197	7999.757322	10.001741	-0.055790	4.815452
273.181469	7999.801282	10.006746	-0.055804	4.815464
273.274833	7999.864748	10.011751	-0.055821	4.815483
273.189291	7999.792840	10.016755	-0.055805	4.815462
273.470916	7999.773937	10.021760	-0.055857	4.815455
273.235338	7999.881154	10.026765	-0.055813	4.815488
273.216710	7999.793251	10.031770	-0.055809	4.815462
273.076627	7999.772789	10.036775	-0.055783	4.815457
273.190544	7999.802411	10.041779	-0.055804	4.815465
273.387359	7999.792802	10.046784	-0.055841	4.815461
273.251044	7999.773469	10.051789	-0.055815	4.815456
273.330355	7999.810002	10.056794	-0.055830	4.815466
273.377919	7999.882332	10.061799	-0.055839	4.815487
273.367876	7999.774275	10.066803	-0.055837	4.815456
273.211319	7999.774905	10.071808	-0.055807	4.815457
273.109464	7999.767885	10.076813	-0.055788	4.815455
273.374338	7999.804250	10.081818	-0.055837	4.815464
273.295788	7999.883061	10.086823	-0.055823	4.815488
273.241334	7999.806321	10.091827	-0.055812	4.815466
273.227152	7999.787919	10.096832	-0.055810	4.815460
273.289731	7999.866903	10.101837	-0.055821	4.815483
273.216468	7999.797332	10.106842	-0.055807	4.815463
273.173885	7999.757102	10.111847	-0.055799	4.815452
273.337460	7999.798218	10.116851	-0.055830	4.815463
273.258198	7999.885563	10.121856	-0.055815	4.815489
273.399565	7999.759689	10.126861	-0.055841	4.815451
273.539949	7999.795086	10.131866	-0.055867	4.815461
273.520000	7999.762703	10.136871	-0.055863	4.815452
273.494985	7999.882979	10.141875	-0.055858	4.815487
273.515263	7999.779690	10.146880	-0.055862	4.815457
273.445267	7999.794554	10.151885	-0.055849	4.815461
273.523373	7999.883406	10.156890	-0.055863	4.815487
273.494884	7999.798545	10.161895	-0.055858	4.815462
273.505529	7999.790162	10.166899	-0.055859	4.815460
273.385505	7999.869363	10.171904	-0.055837	4.815483
273.278890	7999.770407	10.176909	-0.055817	4.815455
273.631733	7999.815688	10.181914	-0.055883	4.815467
273.526083	7999.800061	10.186919	-0.055863	4.815463
273.455043	7999.798886	10.191923	-0.055849	4.815463
273.707991	7999.807286	10.196928	-0.055896	4.815464
273.599729	7999.871725	10.201933	-0.055876	4.815483
273.535515	7999.784144	10.206938	-0.055864	4.815458
273.610934	7999.794979	10.211943	-0.055878	4.815461
273.656938	7999.804264	10.216947	-0.055886	4.815463
273.550274	7999.816391	10.221952	-0.055866	4.815467
273.547925	7999.770411	10.226957	-0.055866	4.815454
273.715621	7999.824413	10.231962	-0.055897	4.815469
273.468557	7999.859878	10.236967	-0.055851	4.815480
273.476145	7999.782017	10.241971	-0.055852	4.815458
273.606599	7999.779866	10.246976	-0.055876	4.815456
273.584720	7999.864946	10.251981	-0.055872	4.815481
273.708682	7999.809283	10.256986	-0.055895	4.815464
273.491100	7999.789688	10.261991	-0.055854	4.815460
273.745129	7999.795969	10.266995	-0.055901	4.815460
273.568598	7999.821907	10.272000	-0.055868	4.815469
273.486690	7999.789578	10.277005	-0.055853	4.815460
273.766186	7999.795208	10.282010	-0.055905	4.815460
273.660271	7999.847936	10.287015	-0.055885	4.815476
273.673787	7999.872712	10.292019	-0.055887	4.815483
273.679088	7999.804426	10.297024	-0.055888	4.815463
273.647422	7999.856233	10.302029	-0.055882	4.815478
273.683242	7999.766016	10.307034	-0.055889	4.815452
273.593150	7999.990973	10.312039	-0.055872	4.815518
273.611370	7999.899399	10.317043	-0.055875	4.815491
273.824835	7999.870836	10.322048	-0.055915	4.815482
273.618365	7999.865308	10.327053	-0.055876	4.815481
273.771884	7999.785563	10.332058	-0.055904	4.815457
273.718063	7999.775056	10.337063	-0.055894	4.815454
273.470969	7999.856450	10.342067	-0.055848	4.815479
273.818475	7999.787356	10.347072	-0.055913	4.815458
273.668942	7999.764602	10.352077	-0.055885	4.815452
273.557904	7999.814042	10.357082	-0.055864	4.815467
273.506990	7999.855921	10.362087	-0.055854	4.815479
273.630102	7999.773541	10.367091	-0.055877	4.815454
273.716374	7999.797371	10.372096	-0.055893	4.815461
273.547250	7999.870428	10.377101	-0.055861	4.815483
273.722995	7999.795318	10.382106	-0.055894	4.815460
273.687317	7999.773360	10.387111	-0.055887	4.815454
273.503387	7999.809858	10.392115	-0.055853	4.815466
273.641716	7999.788610	10.397120	-0.055878	4.815459
273.641501	7999.769368	10.402125	-0.055878	4.815453
273.858391	7999.877581	10.407130	-0.055918	4.815484
273.713984	7999.804709	10.412135	-0.055891	4.815463
273.834667	7999.779968	10.417139	-0.055914	4.815455
273.722738	7999.806963	10.422144	-0.055893	4.815464
273.482433	7999.775247	10.427149	-0.055848	4.815456
273.599464	7999.783558	10.432154	-0.055869	4.815458
273.645239	7999.857996	10.437159	-0.055878	4.815479
273.613453	7999.772013	10.442163	-0.055872	4.815454
273.807375	7999.780515	10.447168	-0.055908	4.815456
273.873629	7999.872377	10.452173	-0.055920	4.815482
273.726345	7999.813343	10.457178	-0.055892	4.815466
273.521900	7999.805713	10.462183	-0.055854	4.815464
273.926059	7999.793088	10.467187	-0.055929	4.815459
273.937483	7999.794331	10.472192	-0.055931	4.815459
273.575789	7999.848214	10.477197	-0.055864	4.815477
273.698239	7999.872636	10.482202	-0.055886	4.815483
273.779533	7999.754324	10.487207	-0.055901	4.815448
273.725997	7999.864520	10.492211	-0.055891	4.815481
273.718809	7999.801371	10.497216	-0.055890	4.815462
273.785542	7999.778951	10.502221	-0.055902	4.815455
273.968417	7999.822521	10.507226	-0.055936	4.815467
273.699741	7999.872585	10.512231	-0.055886	4.815483
273.560117	7999.773089	10.517235	-0.055860	4.815455
273.691234	7999.783767	10.522240	-0.055884	4.815457
273.661608	7999.866583	10.527245	-0.055878	4.815482
273.687073	7999.800763	10.532250	-0.055883	4.815462
273.864678	7999.785499	10.537255	-0.055916	4.815457
273.603921	7999.788696	10.542259	-0.055867	4.815459
273.741442	7999.893475	10.547264	-0.055893	4.815489
273.688357	7999.792189	10.552269	-0.055882	4.815460
273.668570	7999.840987	10.557274	-0.055879	4.815474
273.616212	7999.786711	10.562279	-0.055869	4.815459
273.667765	7999.767248	10.567283	-0.055878	4.815453
273.909026	7999.903632	10.572288	-0.055923	4.815491
273.688450	7999.759016	10.577293	-0.055882	4.815450
273.754981	7999.794273	10.582298	-0.055894	4.815460
273.836444	7999.792389	10.587303	-0.055909	4.815459
273.922300	7999.800190	10.592307	-0.055925	4.815461
273.685371	7999.889227	10.597312	-0.055881	4.815488
273.769700	7999.749602	10.602317	-0.055896	4.815447
273.824053	7999.783591	10.607322	-0.055906	4.815457
273.615323	7999.795116	10.612327	-0.055867	4.815461
273.615913	7999.890177	10.617331	-0.055867	4.815489
273.993572	7999.814099	10.622336	-0.055937	4.815465
273.665043	7999.778802	10.627341	-0.055876	4.815456
273.732162	7999.878156	10.632346	-0.055888	4.815485
273.709319	7999.766685	10.637351	-0.055884	4.815452
273.815041	7999.854920	10.642355	-0.055904	4.815478
273.808003	7999.778956	10.647360	-0.055902	4.815455
273.824944	7999.865739	10.652365	-0.055905	4.815481
273.942169	7999.781126	10.657370	-0.055927	4.815455
273.983386	7999.788197	10.662375	-0.055934	4.815457
273.789229	7999.865117	10.667379	-0.055898	4.815481
273.924541	7999.785073	10.672384	-0.055923	4.815457
273.767737	7999.878625	10.677389	-0.055894	4.815485
273.711954	7999.784773	10.682394	-0.055883	4.815458
273.709733	7999.784724	10.687399	-0.055883	4.815458
273.848840	7999.780579	10.692403	-0.055908	4.815456
273.946003	7999.791770	10.697408	-0.055926	4.815459
273.693583	7999.778014	10.702413	-0.055879	4.815456
274.014223	7999.802475	10.707418	-0.055939	4.815461
273.948943	7999.817416	10.712423	-0.055926	4.815466
273.722571	7999.899149	10.717427	-0.055884	4.815491
273.931144	7999.801077	10.722432	-0.055923	4.815461
273.869745	7999.777629	10.727437	-0.055911	4.815455
273.925550	7999.800961	10.732442	-0.055922	4.815461
273.949002	7999.861147	10.737447	-0.055926	4.815479
273.817035	7999.782070	10.742451	-0.055901	4.815456
273.940616	7999.880212	10.747456	-0.055924	4.815484
273.790686	7999.865996	10.752461	-0.055896	4.815481
273.879667	7999.796943	10.757466	-0.055912	4.815460
273.892483	7999.782186	10.762471	-0.055915	4.815456
273.862381	7999.881017	10.767475	-0.055909	4.815485
273.930147	7999.780641	10.772480	-0.055921	4.815455
273.987194	7999.793312	10.777485	-0.055932	4.815459
273.881342	7999.805453	10.782490	-0.055912	4.815463
273.885899	7999.822605	10.787495	-0.055913	4.815468
273.902873	7999.802576	10.792499	-0.055916	4.815462
273.866648	7999.816924	10.797504	-0.055909	4.815466
273.772312	7999.780119	10.802509	-0.055891	4.815456
273.931201	7999.775230	10.807514	-0.055920	4.815454
274.045549	7999.898856	10.812519	-0.055942	4.815489
273.834221	7999.791776	10.817523	-0.055902	4.815459
273.820500	7999.799016	10.822528	-0.055899	4.815461
273.921371	7999.783564	10.827533	-0.055918	4.815456
273.799146	7999.825345	10.832538	-0.055895	4.815469
273.826131	7999.796934	10.837543	-0.055900	4.815461
273.918301	7999.782408	10.842547	-0.055917	4.815456
273.897068	7999.802343	10.847552	-0.055913	4.815462
273.894791	7999.795884	10.852557	-0.055912	4.815460
273.902278	7999.881445	10.857562	-0.055914	4.815485
273.997895	7999.787933	10.862567	-0.055931	4.815457
273.764364	7999.856732	10.867571	-0.055888	4.815478
273.875219	7999.825421	10.872576	-0.055908	4.815469
273.908383	7999.768273	10.877581	-0.055914	4.815452
273.987967	7999.801607	10.882586	-0.055929	4.815461
274.056103	7999.789892	10.887591	-0.055941	4.815458
274.117155	7999.856034	10.892595	-0.055953	4.815477
273.983849	7999.807910	10.897600	-0.055928	4.815463
273.846100	7999.771463	10.902605	-0.055902	4.815453
273.867146	7999.808112	10.907610	-0.055906	4.815464
274.005954	7999.792213	10.912615	-0.055931	4.815459
273.883370	7999.794466	10.917619	-0.055908	4.815460
273.897567	7999.901499	10.922624	-0.055911	4.815491
273.972248	7999.763852	10.927629	-0.055925	4.815450
274.003316	7999.781438	10.932634	-0.055930	4.815455
274.118495	7999.862352	10.937639	-0.055952	4.815478
273.912167	7999.793807	10.942643	-0.055913	4.815459
274.063830	7999.817639	10.947648	-0.055941	4.815466
273.837390	7999.791490	10.952653	-0.055899	4.815459
274.105700	7999.819368	10.957658	-0.055949	4.815466
274.155498	7999.799876	10.962663	-0.055958	4.815460
274.063314	7999.799422	10.967667	-0.055940	4.815460
274.247143	7999.802419	10.972672	-0.055975	4.815460
274.019251	7999.861696	10.977677	-0.055932	4.815479
273.896704	7999.793454	10.982682	-0.055909	4.815459
273.925212	7999.793908	10.987687	-0.055914	4.815459
274.053317	7999.886783	10.992691	-0.055938	4.815486
274.130869	7999.819679	10.997696	-0.055952	4.815466
273.932172	7999.779030	11.002701	-0.055915	4.815455
273.937076	7999.779098	11.007706	-0.055916	4.815455
274.217321	7999.802898	11.012711	-0.055968	4.815461
274.108576	7999.780811	11.017715	-0.055947	4.815455
274.186570	7999.901707	11.022720	-0.055962	4.815490
273.888081	7999.771837	11.027725	-0.055906	4.815453
273.930564	7999.799223	11.032730	-0.055914	4.815461
274.074506	7999.790885	11.037735	-0.055941	4.815458
274.055242	7999.787353	11.042739	-0.055937	4.815457
274.074286	7999.834650	11.047744	-0.055940	4.815471
274.147190	7999.808059	11.052749	-0.055954	4.815463
274.035698	7999.822244	11.057754	-0.055933	4.815467
274.124519	7999.814072	11.062759	-0.055949	4.815464
274.055739	7999.788366	11.067763	-0.055936	4.815457
273.968315	7999.872374	11.072768	-0.055920	4.815482
274.145179	7999.776988	11.077773	-0.055953	4.815454
274.134238	7999.775728	11.082778	-0.055950	4.815453
273.981064	7999.872545	11.087783	-0.055922	4.815482
273.902184	7999.873377	11.092787	-0.055907	4.815483
274.159169	7999.783575	11.097792	-0.055955	4.815455
273.950981	7999.767338	11.102797	-0.055916	4.815452
273.847925	7999.781661	11.107802	-0.055896	4.815456
274.075821	7999.874033	11.112807	-0.055939	4.815482
274.160610	7999.760050	11.117811	-0.055954	4.815449
273.969877	7999.794300	11.122816	-0.055919	4.815459
273.963727	7999.876433	11.127821	-0.055917	4.815483
274.097239	7999.801700	11.132826	-0.055942	4.815461
274.005470	7999.809799	11.137831	-0.055925	4.815464
274.006535	7999.873892	11.142835	-0.055925	4.815483
274.244767	7999.835053	11.147840	-0.055969	4.815470
273.922334	7999.787038	11.152845	-0.055909	4.815458
274.114943	7999.833971	11.157850	-0.055945	4.815470
274.205676	7999.840785	11.162855	-0.055961	4.815472
274.243072	7999.801863	11.167859	-0.055968	4.815460
274.170382	7999.830569	11.172864	-0.055955	4.815469
274.089237	7999.797184	11.177869	-0.055939	4.815460
274.099209	7999.794130	11.182874	-0.055941	4.815459
274.112968	7999.809297	11.187879	-0.055943	4.815463
274.027632	7999.790798	11.192883	-0.055927	4.815458
274.277234	7999.841868	11.197888	-0.055974	4.815472
273.924428	7999.796560	11.202893	-0.055908	4.815460
273.903439	7999.821839	11.207898	-0.055904	4.815468
274.175136	7999.892498	11.212903	-0.055954	4.815487
274.092521	7999.762957	11.217907	-0.055939	4.815450
274.017151	7999.793755	11.222912	-0.055925	4.815459
274.182653	7999.868017	11.227917	-0.055955	4.815480
274.179601	7999.798525	11.232922	-0.055955	4.815460
274.157288	7999.835532	11.237927	-0.055950	4.815471
274.247504	7999.810293	11.242931	-0.055967	4.815463
274.212541	7999.823594	11.247936	-0.055960	4.815467
274.170785	7999.794058	11.252941	-0.055952	4.815459
274.039612	7999.817534	11.257946	-0.055928	4.815466
274.133230	7999.815849	11.262951	-0.055945	4.815465
274.066842	7999.877770	11.267955	-0.055933	4.815483
274.121910	7999.812435	11.272960	-0.055943	4.815464
274.149407	7999.787237	11.277965	-0.055948	4.815457
274.148530	7999.785074	11.282970	-0.055947	4.815456
274.169721	7999.795021	11.287975	-0.055951	4.815459
273.961803	7999.791606	11.292979	-0.055912	4.815459
274.102490	7999.807782	11.297984	-0.055938	4.815463
274.176408	7999.873067	11.302989	-0.055952	4.815482
274.085975	7999.798941	11.307994	-0.055935	4.815460
274.181401	7999.842148	11.312999	-0.055953	4.815473
274.228632	7999.807660	11.318003	-0.055961	4.815462
274.249326	7999.802645	11.323008	-0.055965	4.815461
273.985548	7999.778021	11.328013	-0.055916	4.815455
274.146945	7999.797740	11.333018	-0.055946	4.815460
274.158006	7999.805386	11.338023	-0.055948	4.815462
273.972557	7999.864289	11.343027	-0.055913	4.815480
274.149013	7999.803077	11.348032	-0.055946	4.815461
274.221719	7999.810663	11.353037	-0.055959	4.815463
274.011424	7999.812550	11.358042	-0.055920	4.815465
274.172133	7999.849348	11.363047	-0.055950	4.815475
274.326217	7999.787769	11.368051	-0.055978	4.815456
274.363418	7999.819342	11.373056	-0.055985	4.815465
274.237922	7999.800185	11.378061	-0.055961	4.815460
274.253190	7999.803626	11.383066	-0.055964	4.815461
274.250598	7999.812117	11.388071	-0.055963	4.815464
274.126686	7999.789781	11.393075	-0.055940	4.815458
274.362882	7999.838497	11.398080	-0.055984	4.815471
274.207829	7999.873331	11.403085	-0.055955	4.815482
274.037252	7999.807506	11.408090	-0.055923	4.815463
274.106691	7999.812903	11.413095	-0.055936	4.815464
274.170811	7999.780828	11.418099	-0.055948	4.815455
274.197261	7999.830382	11.423104	-0.055952	4.815469
274.366030	7999.802156	11.428109	-0.055984	4.815460
274.263827	7999.804743	11.433114	-0.055965	4.815461
274.286404	7999.838213	11.438119	-0.055969	4.815471
274.135400	7999.891271	11.443123	-0.055940	4.815487
274.210587	7999.818788	11.448128	-0.055954	4.815466
274.319234	7999.789578	11.453133	-0.055974	4.815457
274.023590	7999.812498	11.458138	-0.055919	4.815465
274.194269	7999.852664	11.463143	-0.055951	4.815476
274.261289	7999.800342	11.468147	-0.055963	4.815460
274.371812	7999.841659	11.473152	-0.055984	4.815472
274.280672	7999.789952	11.478157	-0.055966	4.815457
274.380686	7999.802258	11.483162	-0.055985	4.815460
274.490426	7999.805110	11.488167	-0.056005	4.815460
274.217218	7999.787808	11.493171	-0.055954	4.815457
274.275063	7999.827195	11.498176	-0.055965	4.815468
274.398976	7999.807848	11.503181	-0.055988	4.815462
274.387878	7999.888833	11.508186	-0.055986	4.815485
274.344704	7999.808003	11.513191	-0.055977	4.815462
274.175448	7999.783857	11.518195	-0.055946	4.815456
274.252293	7999.836373	11.523200	-0.055960	4.815471
274.069426	7999.823754	11.528205	-0.055926	4.815468
274.087713	7999.825109	11.533210	-0.055929	4.815468
274.200703	7999.857922	11.538215	-0.055950	4.815477
274.098103	7999.786801	11.543219	-0.055931	4.815457
274.258119	7999.811839	11.548224	-0.055960	4.815464
274.321858	7999.858799	11.553229	-0.055972	4.815477
274.168155	7999.792183	11.558234	-0.055943	4.815458
274.171417	7999.782611	11.563239	-0.055944	4.815455
274.358416	7999.770705	11.568243	-0.055978	4.815451
274.340989	7999.818473	11.573248	-0.055975	4.815465
274.164163	7999.809158	11.578253	-0.055942	4.815463
274.480776	7999.816464	11.583258	-0.056001	4.815464
274.622623	7999.815569	11.588263	-0.056027	4.815463
274.227041	7999.805877	11.593267	-0.055953	4.815462
274.226520	7999.829355	11.598272	-0.055953	4.815469
274.452645	7999.776432	11.603277	-0.055995	4.815452
274.333987	7999.959266	11.608282	-0.055973	4.815506
274.205108	7999.784105	11.613287	-0.055948	4.815456
274.118564	7999.938623	11.618291	-0.055932	4.815501
274.152920	7999.787498	11.623296	-0.055938	4.815457
273.998421	7999.761458	11.628301	-0.055910	4.815450
274.291049	7999.847413	11.633306	-0.055964	4.815474
274.362243	7999.778069	11.638311	-0.055977	4.815453
274.333646	7999.873721	11.643315	-0.055972	4.815481
274.304663	7999.795260	11.648320	-0.055966	4.815459
274.362627	7999.778038	11.653325	-0.055977	4.815453
274.181939	7999.898971	11.658330	-0.055943	4.815489
274.099701	7999.811094	11.663335	-0.055927	4.815464
274.096211	7999.769367	11.668339	-0.055927	4.815452
274.191671	7999.788007	11.673344	-0.055944	4.815457
274.158736	7999.775706	11.678349	-0.055938	4.815454
274.253376	7999.886192	11.683354	-0.055956	4.815485
274.371051	7999.793042	11.688359	-0.055977	4.815458
274.138874	7999.856521	11.693363	-0.055934	4.815477
274.156533	7999.798051	11.698368	-0.055937	4.815460
274.304030	7999.799384	11.703373	-0.055964	4.815460
274.152450	7999.852434	11.708378	-0.055936	4.815476
274.114122	7999.824022	11.713383	-0.055929	4.815468
274.089963	7999.774480	11.718387	-0.055924	4.815454
274.293227	7999.808770	11.723392	-0.055962	4.815463
274.063351	7999.798587	11.728397	-0.055919	4.815461
274.229221	7999.805561	11.733402	-0.055950	4.815462
274.291429	7999.825794	11.738407	-0.055961	4.815468
274.118741	7999.794115	11.743411	-0.055929	4.815459
274.258204	7999.800658	11.748416	-0.055955	4.815460
274.314144	7999.905170	11.753421	-0.055965	4.815491
274.158125	7999.819289	11.758426	-0.055936	4.815466
274.159797	7999.859893	11.763431	-0.055936	4.815478
274.056920	7999.815471	11.768435	-0.055916	4.815466
274.136497	7999.843464	11.773440	-0.055931	4.815473
274.180266	7999.795034	11.778445	-0.055939	4.815459
274.083254	7999.789161	11.783450	-0.055921	4.815458
274.216680	7999.783856	11.788455	-0.055946	4.815456
274.080938	7999.847846	11.793459	-0.055920	4.815475
274.243015	7999.777853	11.798464	-0.055950	4.815454
274.458550	7999.816617	11.803469	-0.055990	4.815464
274.499296	7999.816203	11.808474	-0.055998	4.815464
274.200740	7999.802759	11.813479	-0.055942	4.815461
274.052027	7999.852650	11.818483	-0.055914	4.815477
274.201444	7999.784587	11.823488	-0.055942	4.815456
274.212602	7999.869139	11.828493	-0.055944	4.815481
274.139298	7999.788885	11.833498	-0.055930	4.815458
274.295863	7999.804253	11.838503	-0.055959	4.815461
274.311262	7999.867512	11.843507	-0.055962	4.815480
274.225641	7999.780648	11.848512	-0.055946	4.815455
274.293059	7999.869326	11.853517	-0.055958	4.815480
274.407272	7999.784664	11.858522	-0.055979	4.815455
274.277120	7999.808156	11.863527	-0.055955	4.815463
274.054184	7999.784200	11.868531	-0.055913	4.815457
274.376216	7999.889863	11.873536	-0.055973	4.815486
274.313532	7999.769193	11.878541	-0.055961	4.815451
274.027436	7999.878788	11.883546	-0.055908	4.815484
274.273407	7999.784534	11.888551	-0.055953	4.815456
274.262796	7999.861253	11.893555	-0.055951	4.815478
274.152348	7999.801754	11.898560	-0.055931	4.815461
274.180096	7999.832103	11.903565	-0.055936	4.815470
274.237705	7999.819148	11.908570	-0.055946	4.815466
274.248321	7999.834263	11.913575	-0.055948	4.815470
274.024942	7999.801755	11.918579	-0.055906	4.815462
274.307268	7999.927062	11.923584	-0.055959	4.815497
274.270317	7999.774770	11.928589	-0.055952	4.815453
274.140166	7999.768354	11.933594	-0.055927	4.815452
274.223298	7999.880788	11.938599	-0.055943	4.815484
274.188690	7999.852438	11.943603	-0.055936	4.815476
274.170115	7999.884165	11.948608	-0.055932	4.815485
274.133651	7999.779947	11.953613	-0.055925	4.815455
274.120151	7999.873709	11.958618	-0.055923	4.815483
274.406985	7999.796145	11.963623	-0.055976	4.815459
274.249619	7999.765786	11.968627	-0.055947	4.815450
274.287622	7999.867868	11.973632	-0.055954	4.815480
274.394833	7999.859997	11.978637	-0.055973	4.815477
274.220745	7999.779161	11.983642	-0.055941	4.815454
274.423327	7999.776056	11.988647	-0.055978	4.815453
274.542697	7999.864516	11.993651	-0.056001	4.815478
274.532644	7999.856862	11.998656	-0.055999	4.815476
274.314789	7999.810558	12.003661	-0.055958	4.815463
274.425480	7999.878582	12.008666	-0.055978	4.815483
274.466450	7999.799130	12.013671	-0.055986	4.815459
274.380377	7999.774209	12.018675	-0.055970	4.815452
274.343269	7999.801361	12.023680	-0.055963	4.815460
274.511694	7999.796628	12.028685	-0.055994	4.815458
274.349523	7999.799302	12.033690	-0.055963	4.815460
274.241886	7999.812481	12.038695	-0.055943	4.815464
274.194999	7999.781794	12.043699	-0.055934	4.815455
274.302817	7999.885019	12.048704	-0.055954	4.815485
274.329745	7999.812814	12.053709	-0.055959	4.815464
274.290381	7999.788658	12.058714	-0.055952	4.815457
274.407539	7999.798040	12.063719	-0.055973	4.815459
274.082584	7999.782028	12.068723	-0.055913	4.815456
274.353278	7999.892191	12.073728	-0.055963	4.815487
274.275636	7999.771276	12.078733	-0.055948	4.815452
274.179983	7999.863694	12.083738	-0.055930	4.815479
274.379863	7999.816751	12.088743	-0.055968	4.815465
274.319140	7999.764474	12.093747	-0.055956	4.815450
274.282927	7999.820480	12.098752	-0.055949	4.815466
274.342063	7999.872706	12.103757	-0.055960	4.815481
274.291565	7999.781075	12.108762	-0.055950	4.815455
274.504645	7999.787755	12.113767	-0.055990	4.815456
274.351961	7999.864285	12.118771	-0.055961	4.815479
274.192618	7999.807190	12.123776	-0.055932	4.815463
274.401682	7999.763601	12.128781	-0.055970	4.815449
274.414113	7999.881287	12.133786	-0.055973	4.815483
274.501822	7999.771624	12.138791	-0.055989	4.815451
274.429745	7999.759750	12.143795	-0.055975	4.815448
274.467501	7999.805217	12.148800	-0.055982	4.815461
274.353610	7999.808681	12.153805	-0.055961	4.815463
274.211454	7999.908883	12.158810	-0.055934	4.815493
274.406813	7999.821277	12.163815	-0.055970	4.815466
274.359911	7999.772430	12.168819	-0.055961	4.815452
274.329229	7999.790074	12.173824	-0.055956	4.815457
274.399835	7999.783740	12.178829	-0.055969	4.815455
274.209956	7999.866070	12.183834	-0.055933	4.815480
274.308993	7999.805727	12.188839	-0.055951	4.815462
274.287857	7999.767984	12.193843	-0.055947	4.815451
274.346032	7999.825535	12.198848	-0.055958	4.815468
274.430982	7999.822640	12.203853	-0.055974	4.815466
274.319783	7999.790900	12.208858	-0.055953	4.815458
274.574863	7999.796130	12.213863	-0.056000	4.815458
274.425072	7999.802211	12.218867	-0.055972	4.815460
274.318120	7999.814334	12.223872	-0.055952	4.815464
274.392487	7999.915944	12.228877	-0.055966	4.815494
274.409730	7999.789105	12.233882	-0.055969	4.815457
274.414676	7999.807331	12.238887	-0.055970	4.815462
274.329056	7999.862529	12.243891	-0.055954	4.815478
274.556813	7999.814974	12.248896	-0.055996	4.815464
274.436695	7999.801246	12.253901	-0.055973	4.815460
274.273326	7999.786810	12.258906	-0.055943	4.815457
274.489778	7999.833065	12.263911	-0.055983	4.815469
274.577921	7999.778952	12.268915	-0.055999	4.815453
274.449241	7999.891124	12.273920	-0.055975	4.815486
274.639895	7999.777806	12.278925	-0.056010	4.815452
274.451243	7999.778978	12.283930	-0.055975	4.815454
274.444019	7999.891001	12.288935	-0.055974	4.815486
274.485744	7999.782722	12.293939	-0.055981	4.815454
274.438390	7999.818251	12.298944	-0.055972	4.815465
274.554511	7999.779550	12.303949	-0.055994	4.815453
274.377064	7999.790518	12.308954	-0.055961	4.815457
274.456180	7999.837731	12.313959	-0.055975	4.815471
274.414458	7999.865875	12.318963	-0.055967	4.815479
274.405097	7999.802689	12.323968	-0.055965	4.815461
274.604269	7999.815550	12.328973	-0.056002	4.815464
274.560796	7999.775305	12.333978	-0.055994	4.815452
274.709798	7999.818321	12.338983	-0.056022	4.815464
274.669641	7999.886012	12.343987	-0.056014	4.815484
274.679552	7999.840231	12.348992	-0.056016	4.815470
274.628400	7999.845790	12.353997	-0.056006	4.815472
274.432446	7999.829753	12.359002	-0.055970	4.815468
274.536269	7999.838916	12.364007	-0.055989	4.815471
274.590862	7999.782118	12.369011	-0.055999	4.815454
274.413137	7999.767447	12.374016	-0.055966	4.815450
274.585604	7999.798029	12.379021	-0.055998	4.815459
274.503498	7999.777446	12.384026	-0.055982	4.815453
274.516093	7999.803275	12.389031	-0.055984	4.815460
274.473084	7999.892282	12.394035	-0.055976	4.815487
274.556186	7999.818860	12.399040	-0.055992	4.815465
274.525668	7999.796985	12.404045	-0.055986	4.815459
274.400000	7999.782098	12.409050	-0.055962	4.815455
274.653536	7999.809735	12.414055	-0.056009	4.815462
274.449591	7999.786089	12.419059	-0.055971	4.815456
274.328624	7999.775552	12.424064	-0.055948	4.815453
274.468169	7999.795981	12.429069	-0.055974	4.815459
274.570332	7999.868138	12.434074	-0.055993	4.815479
274.490837	7999.797396	12.439079	-0.055978	4.815459
274.341528	7999.770372	12.444083	-0.055950	4.815452
274.455397	7999.873696	12.449088	-0.055971	4.815481
274.621738	7999.768525	12.454093	-0.056002	4.815450
274.354262	7999.767339	12.459098	-0.055952	4.815451
274.589872	7999.819249	12.464103	-0.055996	4.815465
274.534347	7999.808714	12.469107	-0.055985	4.815462
274.525177	7999.892934	12.474112	-0.055984	4.815487
274.514906	7999.775258	12.479117	-0.055982	4.815452
274.446620	7999.765583	12.484122	-0.055969	4.815450
274.455983	7999.891764	12.489127	-0.055970	4.815487
274.544937	7999.785326	12.494131	-0.055987	4.815455
274.528005	7999.781832	12.499136	-0.055983	4.815454
274.560521	7999.834690	12.504141	-0.055989	4.815469
274.462809	7999.789284	12.509146	-0.055971	4.815457
274.532502	7999.819252	12.514151	-0.055984	4.815465
274.623808	7999.864528	12.519155	-0.056001	4.815478
274.681428	7999.781076	12.524160	-0.056011	4.815453
274.579303	7999.806095	12.529165	-0.055992	4.815461
274.519887	7999.799769	12.534170	-0.055981	4.815459
274.640433	7999.956611	12.539175	-0.056003	4.815505
274.568584	7999.789860	12.544179	-0.055990	4.815456
274.519182	7999.796516	12.549184	-0.055980	4.815459
274.942836	7999.775667	12.554189	-0.056059	4.815450
274.500744	7999.790848	12.559194	-0.055977	4.815457
274.544775	7999.817192	12.564199	-0.055985	4.815464
274.796151	7999.795659	12.569203	-0.056031	4.815457
274.518283	7999.829551	12.574208	-0.055979	4.815468
274.588193	7999.797570	12.579213	-0.055992	4.815459
274.417242	7999.793691	12.584218	-0.055960	4.815458
274.574826	7999.847529	12.589223	-0.055990	4.815473
274.507027	7999.826112	12.594227	-0.055977	4.815467
274.504720	7999.902968	12.599232	-0.055976	4.815490
274.690098	7999.777813	12.604237	-0.056011	4.815452
274.482139	7999.890823	12.609242	-0.055972	4.815486
274.592631	7999.836008	12.614247	-0.055992	4.815470
274.715283	7999.825186	12.619251	-0.056015	4.815466
274.435495	7999.823798	12.624256	-0.055963	4.815467
274.489182	7999.816119	12.629261	-0.055972	4.815464
274.404827	7999.779477	12.634266	-0.055957	4.815454
274.493554	7999.790530	12.639271	-0.055973	4.815457
274.553247	7999.773336	12.644275	-0.055984	4.815452
274.537542	7999.868131	12.649280	-0.055981	4.815479
274.760180	7999.778835	12.654285	-0.056022	4.815452
274.670323	7999.884166	12.659290	-0.056005	4.815483
274.551496	7999.823460	12.664295	-0.055983	4.815466
274.486156	7999.788197	12.669299	-0.055971	4.815456
274.458217	7999.778114	12.674304	-0.055965	4.815454
274.538120	7999.787955	12.679309	-0.055980	4.815456
274.662815	7999.956614	12.684314	-0.056003	4.815505
274.678239	7999.803041	12.689319	-0.056006	4.815460
274.680999	7999.794529	12.694323	-0.056006	4.815457
274.480102	7999.813658	12.699328	-0.055969	4.815464
274.498602	7999.791518	12.704333	-0.055972	4.815457
274.493167	7999.781803	12.709338	-0.055971	4.815454
274.564967	7999.808601	12.714343	-0.055984	4.815462
274.834467	7999.878157	12.719347	-0.056034	4.815481
274.597474	7999.805904	12.724352	-0.055990	4.815461
274.444034	7999.814061	12.729357	-0.055961	4.815464
274.404725	7999.796315	12.734362	-0.055954	4.815459
274.628306	7999.811712	12.739367	-0.055995	4.815463
274.561038	7999.780690	12.744371	-0.055983	4.815454
274.531147	7999.946818	12.749376	-0.055977	4.815503
274.675751	7999.801769	12.754381	-0.056004	4.815459
274.858146	7999.772698	12.759386	-0.056037	4.815450
274.585698	7999.807747	12.764391	-0.055987	4.815462
274.508034	7999.902596	12.769395	-0.055972	4.815490
274.480032	7999.828423	12.774400	-0.055967	4.815468
274.487792	7999.821061	12.779405	-0.055968	4.815466
274.458386	7999.766092	12.784410	-0.055962	4.815450
274.556049	7999.791177	12.789415	-0.055980	4.815457
274.480553	7999.858290	12.794419	-0.055966	4.815477
274.549467	7999.878632	12.799424	-0.055979	4.815483
274.798709	7999.807929	12.804429	-0.056025	4.815461
274.630715	7999.782736	12.809434	-0.055994	4.815454
274.589741	7999.806620	12.814439	-0.055986	4.815461
274.736379	7999.889118	12.819443	-0.056013	4.815485
274.620991	7999.796425	12.824448	-0.055991	4.815458
274.602393	7999.804653	12.829453	-0.055988	4.815461
274.560428	7999.775114	12.834458	-0.055980	4.815452
274.737962	7999.802575	12.839463	-0.056013	4.815459
274.778319	7999.875857	12.844467	-0.056020	4.815481
274.509911	7999.781726	12.849472	-0.055970	4.815454
274.554897	7999.804881	12.854477	-0.055978	4.815461
274.575430	7999.875702	12.859482	-0.055982	4.815482
274.658390	7999.790528	12.864487	-0.055997	4.815456
274.595426	7999.794826	12.869491	-0.055985	4.815458
274.554875	7999.795217	12.874496	-0.055978	4.815458
274.605014	7999.790685	12.879501	-0.055987	4.815457
274.477487	7999.775767	12.884506	-0.055963	4.815453
274.503323	7999.813562	12.889511	-0.055968	4.815464
274.662950	7999.874911	12.894515	-0.055997	4.815481
274.548247	7999.781160	12.899520	-0.055976	4.815454
274.690116	7999.893489	12.904525	-0.056002	4.815486
274.672779	7999.773561	12.909530	-0.055999	4.815451
274.710808	7999.830782	12.914535	-0.056006	4.815468
274.817528	7999.813290	12.919539	-0.056025	4.815462
274.622735	7999.847474	12.924544	-0.055989	4.815473
274.763541	7999.881810	12.929549	-0.056015	4.815483
274.746418	7999.843064	12.934554	-0.056012	4.815471
274.820010	7999.836780	12.939559	-0.056025	4.815469
274.714832	7999.806205	12.944563	-0.056005	4.815461
274.618916	7999.793941	12.949568	-0.055987	4.815458
274.641796	7999.853051	12.954573	-0.055992	4.815475
274.638018	7999.766457	12.959578	-0.055991	4.815449
274.639128	7999.832688	12.964583	-0.055991	4.815469
274.683264	7999.806694	12.969587	-0.055999	4.815461
274.650157	7999.910818	12.974592	-0.055993	4.815492
274.751855	7999.808860	12.979597	-0.056011	4.815461
274.743938	7999.782014	12.984602	-0.056010	4.815454
274.805215	7999.813981	12.989607	-0.056021	4.815463
274.675048	7999.856700	12.994611	-0.055997	4.815476
274.699151	7999.798334	12.999616	-0.056001	4.815459
274.676852	7999.801161	13.004621	-0.055997	4.815459
274.716636	7999.768687	13.009626	-0.056004	4.815450
274.581077	7999.787818	13.014631	-0.055979	4.815456
274.636797	7999.910486	13.019635	-0.055989	4.815492
274.745751	7999.816124	13.024640	-0.056009	4.815464
274.846525	7999.806012	13.029645	-0.056028	4.815460
274.567429	7999.779000	13.034650	-0.055975	4.815454
274.776512	7999.804841	13.039655	-0.056014	4.815460
274.761631	7999.806721	13.044659	-0.056011	4.815461
274.634002	7999.872980	13.049664	-0.055987	4.815481
274.794040	7999.816840	13.054669	-0.056017	4.815464
274.811126	7999.779722	13.059674	-0.056020	4.815453
274.835334	7999.803605	13.064679	-0.056025	4.815459
275.001746	7999.782817	13.069683	-0.056055	4.815453
274.914894	7999.808087	13.074688	-0.056039	4.815460
274.718226	7999.846512	13.079693	-0.056002	4.815473
274.675658	7999.861825	13.084698	-0.055994	4.815477
274.756679	7999.814004	13.089703	-0.056009	4.815463
274.853216	7999.794209	13.094707	-0.056027	4.815457
274.553972	7999.805320	13.099712	-0.055971	4.815461
274.752183	7999.808552	13.104717	-0.056008	4.815461
274.833085	7999.802387	13.109722	-0.056023	4.815459
274.724826	7999.805943	13.114727	-0.056003	4.815461
274.622522	7999.814937	13.119731	-0.055983	4.815464
274.740077	7999.800827	13.124736	-0.056005	4.815459
274.750846	7999.809536	13.129741	-0.056007	4.815462
274.857922	7999.877501	13.134746	-0.056027	4.815481
275.005259	7999.812607	13.139751	-0.056054	4.815461
274.886290	7999.814920	13.144755	-0.056032	4.815463
274.609578	7999.802901	13.149760	-0.055980	4.815460
274.760171	7999.803217	13.154765	-0.056008	4.815460
274.733441	7999.784608	13.159770	-0.056003	4.815454
274.877395	7999.817928	13.164775	-0.056030	4.815464
274.697099	7999.796806	13.169779	-0.055996	4.815458
274.853863	7999.882675	13.174784	-0.056025	4.815483
275.001828	7999.825269	13.179789	-0.056052	4.815465
274.720693	7999.774724	13.184794	-0.056000	4.815452
274.783197	7999.792825	13.189799	-0.056011	4.815457
274.808008	7999.831671	13.194803	-0.056016	4.815468
274.599281	7999.894467	13.199808	-0.055977	4.815487
274.712079	7999.824735	13.204813	-0.055998	4.815466
274.587579	7999.760733	13.209818	-0.055974	4.815448
274.758047	7999.793418	13.214823	-0.056006	4.815457
274.734525	7999.816520	13.219827	-0.056001	4.815464
274.758295	7999.785920	13.224832	-0.056006	4.815455
274.833714	7999.893957	13.229837	-0.056020	4.815486
274.899938	7999.807441	13.234842	-0.056032	4.815460
275.032399	7999.868345	13.239847	-0.056056	4.815478
274.924395	7999.844133	13.244851	-0.056036	4.815471
274.741625	7999.796266	13.249856	-0.056002	4.815458
274.913531	7999.822567	13.254861	-0.056034	4.815465
274.774858	7999.810671	13.259866	-0.056008	4.815462
274.808819	7999.855008	13.264871	-0.056014	4.815475
274.804775	7999.821817	13.269875	-0.056013	4.815465
274.614019	7999.787706	13.274880	-0.055977	4.815456
274.855365	7999.779895	13.279885	-0.056022	4.815453
274.688101	7999.882890	13.284890	-0.055991	4.815483
274.668343	7999.818466	13.289895	-0.055987	4.815465
274.775123	7999.813792	13.294899	-0.056007	4.815463
274.776076	7999.790296	13.299904	-0.056007	4.815456
274.770966	7999.844675	13.304909	-0.056006	4.815472
274.877222	7999.810085	13.309914	-0.056025	4.815461
275.086544	7999.842340	13.314919	-0.056064	4.815470
274.820342	7999.814470	13.319923	-0.056014	4.815463
274.973894	7999.799881	13.324928	-0.056043	4.815458
275.079062	7999.829362	13.329933	-0.056062	4.815466
274.878860	7999.859184	13.334938	-0.056025	4.815476
274.593826	7999.837415	13.339943	-0.055972	4.815471
274.729711	7999.810787	13.344947	-0.055997	4.815462
274.774528	7999.792282	13.349952	-0.056005	4.815457
274.717567	7999.810563	13.354957	-0.055994	4.815462
274.671598	7999.854660	13.359962	-0.055986	4.815475
274.824997	7999.816569	13.364967	-0.056014	4.815464
274.817529	7999.826048	13.369971	-0.056013	4.815466
274.885983	7999.798316	13.374976	-0.056025	4.815458
274.966548	7999.798554	13.379981	-0.056040	4.815458
274.816581	7999.772588	13.384986	-0.056012	4.815451
274.725103	7999.802054	13.389991	-0.055995	4.815460
274.787005	7999.812668	13.394995	-0.056006	4.815463
274.851320	7999.814776	13.400000	-0.056018	4.815463
274.781358	7999.834981	13.405005	-0.056005	4.815469
274.748150	7999.795972	13.410010	-0.055998	4.815458
274.878736	7999.808779	13.415015	-0.056023	4.815461
274.767012	7999.791983	13.420019	-0.056002	4.815457
274.733194	7999.792485	13.425024	-0.055995	4.815457
275.160766	7999.842198	13.430029	-0.056075	4.815469
275.068806	7999.785137	13.435034	-0.056057	4.815453
274.785990	7999.810402	13.440039	-0.056005	4.815462
274.777733	7999.820936	13.445043	-0.056003	4.815465
274.852134	7999.905457	13.450048	-0.056017	4.815489
274.694211	7999.862269	13.455053	-0.055987	4.815478
274.668431	7999.826586	13.460058	-0.055982	4.815467
274.846601	7999.829490	13.465063	-0.056015	4.815467
274.902799	7999.822921	13.470067	-0.056026	4.815465
274.757308	7999.783142	13.475072	-0.055998	4.815454
274.945373	7999.795821	13.480077	-0.056033	4.815457
275.001912	7999.789257	13.485082	-0.056044	4.815455
274.876731	7999.874783	13.490087	-0.056020	4.815480
274.863125	7999.766665	13.495091	-0.056017	4.815449
275.008239	7999.790391	13.500096	-0.056044	4.815455
274.858260	7999.812491	13.505101	-0.056016	4.815462
274.761701	7999.864304	13.510106	-0.055998	4.815478
274.849040	7999.920197	13.515111	-0.056014	4.815494
275.016256	7999.871651	13.520115	-0.056045	4.815479
274.788996	7999.765377	13.525120	-0.056003	4.815449
274.991672	7999.817816	13.530125	-0.056040	4.815463
274.932421	7999.869173	13.535130	-0.056029	4.815478
274.849016	7999.822933	13.540135	-0.056014	4.815465
274.966140	7999.826974	13.545139	-0.056035	4.815466
275.081929	7999.801085	13.550144	-0.056057	4.815458
275.060348	7999.838105	13.555149	-0.056052	4.815469
274.978672	7999.784416	13.560154	-0.056037	4.815454
275.074117	7999.807329	13.565159	-0.056055	4.815460
275.083711	7999.792519	13.570163	-0.056056	4.815455
274.883042	7999.873605	13.575168	-0.056019	4.815480
275.004851	7999.811498	13.580173	-0.056041	4.815461
275.092874	7999.791563	13.585178	-0.056058	4.815455
275.183256	7999.801576	13.590183	-0.056074	4.815458
274.966857	7999.818315	13.595187	-0.056034	4.815464
274.937874	7999.792193	13.600192	-0.056028	4.815456
274.778270	7999.824816	13.605197	-0.055999	4.815466
274.973716	7999.869661	13.610202	-0.056035	4.815478
275.026414	7999.807491	13.615207	-0.056044	4.815460
275.117383	7999.799354	13.620211	-0.056061	4.815457
274.941222	7999.786844	13.625216	-0.056028	4.815454
275.103836	7999.848242	13.630221	-0.056058	4.815472
275.099856	7999.819324	13.635226	-0.056058	4.815463
275.036570	7999.803322	13.640231	-0.056046	4.815459
275.134720	7999.801711	13.645235	-0.056064	4.815458
275.153109	7999.878907	13.650240	-0.056067	4.815480
275.181067	7999.804581	13.655245	-0.056072	4.815459
275.065294	7999.784515	13.660250	-0.056050	4.815453
275.201235	7999.824113	13.665255	-0.056076	4.815464
275.119566	7999.828104	13.670259	-0.056060	4.815466
274.925835	7999.820648	13.675264	-0.056024	4.815464
274.922177	7999.812030	13.680269	-0.056023	4.815462
275.014519	7999.793235	13.685274	-0.056040	4.815456
275.054618	7999.820582	13.690279	-0.056048	4.815464
274.922206	7999.883559	13.695283	-0.056023	4.815483
275.053510	7999.803449	13.700288	-0.056047	4.815459
275.197876	7999.831435	13.705293	-0.056074	4.815466
275.052624	7999.805545	13.710298	-0.056047	4.815459
274.991535	7999.828032	13.715303	-0.056035	4.815466
275.185831	7999.797020	13.720307	-0.056071	4.815456
275.146044	7999.811310	13.725312	-0.056064	4.815461
274.990407	7999.840794	13.730317	-0.056034	4.815470
275.103890	7999.956931	13.735322	-0.056056	4.815503
274.876223	7999.884829	13.740327	-0.056013	4.815483
274.939981	7999.889065	13.745331	-0.056025	4.815484
274.924044	7999.818294	13.750336	-0.056022	4.815464
274.978681	7999.808495	13.755341	-0.056032	4.815461
274.774273	7999.812613	13.760346	-0.055993	4.815463
274.832945	7999.802879	13.765351	-0.056004	4.815460
275.043708	7999.805249	13.770355	-0.056043	4.815459
274.876271	7999.800359	13.775360	-0.056012	4.815459
274.913458	7999.925928	13.780365	-0.056019	4.815495
275.074892	7999.785427	13.785370	-0.056049	4.815454
274.988287	7999.785065	13.790375	-0.056032	4.815454
275.080951	7999.801523	13.795379	-0.056049	4.815458
274.918005	7999.793503	13.800384	-0.056019	4.815457
274.985647	7999.818097	13.805389	-0.056031	4.815464
274.962214	7999.785656	13.810394	-0.056027	4.815454
274.924220	7999.841633	13.815399	-0.056020	4.815471
275.060060	7999.857731	13.820403	-0.056045	4.815475
274.989417	7999.803154	13.825408	-0.056032	4.815459
274.954805	7999.828210	13.830413	-0.056025	4.815467
275.054976	7999.810611	13.835418	-0.056043	4.815461
274.926618	7999.815974	13.840423	-0.056019	4.815463
275.003706	7999.836450	13.845427	-0.056034	4.815469
275.104551	7999.813522	13.850432	-0.056052	4.815462
275.176646	7999.830712	13.855437	-0.056066	4.815466
274.895485	7999.817551	13.860442	-0.056013	4.815464
274.860024	7999.815890	13.865447	-0.056006	4.815464
274.977497	7999.825277	13.870451	-0.056028	4.815466
274.965766	7999.802642	13.875456	-0.056026	4.815459
274.881209	7999.831153	13.880461	-0.056010	4.815468
274.835572	7999.802622	13.885466	-0.056001	4.815460
274.898518	7999.791890	13.890471	-0.056013	4.815456
274.917269	7999.802866	13.895475	-0.056016	4.815459
274.694991	7999.882530	13.900480	-0.055975	4.815484
274.817939	7999.787329	13.905485	-0.055997	4.815455
274.960489	7999.787514	13.910490	-0.056024	4.815455
274.806087	7999.800996	13.915495	-0.055995	4.815459
274.988684	7999.803972	13.920499	-0.056029	4.815459
274.955278	7999.791663	13.925504	-0.056022	4.815456
274.987229	7999.826354	13.930509	-0.056028	4.815466
275.128159	7999.803013	13.935514	-0.056054	4.815459
275.015844	7999.797958	13.940519	-0.056033	4.815458
274.925444	7999.826373	13.945523	-0.056016	4.815466
274.988008	7999.804954	13.950528	-0.056028	4.815460
275.027197	7999.815196	13.955533	-0.056035	4.815463
274.990422	7999.807105	13.960538	-0.056028	4.815460
275.059289	7999.901149	13.965543	-0.056041	4.815488
275.310507	7999.834751	13.970547	-0.056087	4.815467
275.308750	7999.784507	13.975552	-0.056087	4.815452
275.105371	7999.831368	13.980557	-0.056049	4.815467
275.015462	7999.832019	13.985562	-0.056032	4.815468
275.052304	7999.846496	13.990567	-0.056039	4.815472
274.927879	7999.828424	13.995571	-0.056015	4.815467
274.719874	7999.782281	14.000576	-0.055976	4.815454
274.839442	7999.851519	14.005581	-0.055999	4.815474
275.095746	7999.799090	14.010586	-0.056046	4.815458
274.925626	7999.789884	14.015591	-0.056014	4.815456
274.931246	7999.810258	14.020595	-0.056015	4.815462
274.949429	7999.856474	14.025600	-0.056018	4.815475
274.927171	7999.795213	14.030605	-0.056014	4.815457
274.970929	7999.817279	14.035610	-0.056022	4.815464
275.068249	7999.850904	14.040615	-0.056040	4.815473
275.013305	7999.831834	14.045619	-0.056030	4.815468
274.949199	7999.758138	14.050624	-0.056018	4.815446
275.171923	7999.816247	14.055629	-0.056059	4.815462
275.002241	7999.809184	14.060634	-0.056027	4.815461
274.956709	7999.803085	14.065639	-0.056019	4.815459
274.938961	7999.897847	14.070643	-0.056015	4.815487
275.017497	7999.781624	14.075648	-0.056030	4.815453
274.975708	7999.814040	14.080653	-0.056022	4.815463
274.977023	7999.791618	14.085658	-0.056022	4.815456
275.241336	7999.801273	14.090663	-0.056071	4.815458
274.938279	7999.943704	14.095667	-0.056014	4.815501
274.969949	7999.938869	14.100672	-0.056020	4.815499
274.985321	7999.770341	14.105677	-0.056023	4.815450
275.186878	7999.880443	14.110682	-0.056060	4.815481
275.036008	7999.790372	14.115687	-0.056032	4.815455
275.005184	7999.773833	14.120691	-0.056026	4.815451
275.042738	7999.862023	14.125696	-0.056033	4.815476
275.108190	7999.808607	14.130701	-0.056045	4.815460
275.093830	7999.961105	14.135706	-0.056042	4.815505
275.080156	7999.789964	14.140711	-0.056039	4.815455
275.163281	7999.807335	14.145715	-0.056055	4.815460
275.116233	7999.777712	14.150720	-0.056046	4.815451
275.217101	7999.882961	14.155725	-0.056065	4.815482
275.142262	7999.777045	14.160730	-0.056050	4.815451
275.007343	7999.807936	14.165735	-0.056025	4.815461
275.240389	7999.888646	14.170739	-0.056068	4.815483
275.390072	7999.804564	14.175744	-0.056096	4.815458
275.205659	7999.829304	14.180749	-0.056062	4.815466
275.209434	7999.800513	14.185754	-0.056062	4.815458
275.072598	7999.795056	14.190759	-0.056037	4.815457
275.309529	7999.836308	14.195763	-0.056081	4.815468
275.247287	7999.784005	14.200768	-0.056069	4.815453
275.199233	7999.809909	14.205773	-0.056060	4.815460
275.134772	7999.785342	14.210778	-0.056048	4.815454
274.991522	7999.786189	14.215783	-0.056021	4.815454
275.122362	7999.808613	14.220787	-0.056045	4.815460
275.018419	7999.806899	14.225792	-0.056026	4.815460
275.221259	7999.812343	14.230797	-0.056063	4.815461
275.163887	7999.798574	14.235802	-0.056052	4.815457
275.177686	7999.592636	14.240807	-0.056055	4.815397

275.229447	7996.355207	14.245811	-0.056062	4.814450
275.006058	7990.741672	14.250816	-0.056017	4.812810
275.057493	7983.989463	14.255821	-0.056022	4.810835
275.148085	7976.708373	14.260826	-0.056034	4.808704
275.061710	7969.030045	14.265831	-0.056012	4.806456
274.979717	7961.214751	14.270835	-0.055992	4.804167
275.038715	7953.394720	14.275840	-0.055998	4.801876
274.991733	7945.411799	14.280845	-0.055984	4.799535
274.780525	7937.455896	14.285850	-0.055939	4.797203
274.841614	7929.375001	14.290855	-0.055945	4.794831
274.980790	7921.454423	14.295859	-0.055965	4.792505
274.744163	7913.372904	14.300864	-0.055916	4.790132
274.895320	7905.434760	14.305869	-0.055939	4.787798
274.890144	7897.409104	14.310874	-0.055932	4.785438
274.770493	7889.439957	14.315879	-0.055905	4.783094
274.698471	7881.425575	14.320883	-0.055886	4.780735
274.625040	7873.432123	14.325888	-0.055867	4.778382
274.652172	7865.404770	14.330893	-0.055867	4.776016
274.638337	7857.375569	14.335898	-0.055859	4.773650
274.450834	7849.360853	14.340903	-0.055819	4.771287
274.519677	7841.385135	14.345907	-0.055826	4.768933
274.285375	7833.342989	14.350912	-0.055777	4.766560
274.428020	7825.337000	14.355917	-0.055798	4.764194
274.595482	7817.433466	14.360922	-0.055824	4.761858
274.613864	7809.353592	14.365927	-0.055822	4.759469
274.405371	7801.430259	14.370931	-0.055778	4.757126
274.414638	7793.349928	14.375936	-0.055774	4.754735
274.345231	7785.337087	14.380941	-0.055756	4.752362
274.150317	7777.321637	14.385946	-0.055714	4.749988
274.002154	7769.309729	14.390951	-0.055681	4.747614
274.127063	7761.318471	14.395955	-0.055699	4.745244
274.073449	7753.314582	14.400960	-0.055684	4.742869
274.128980	7745.369469	14.405965	-0.055689	4.740510
274.228402	7737.384599	14.410970	-0.055702	4.738139
274.110149	7729.315427	14.415975	-0.055675	4.735741
274.105380	7721.368023	14.420979	-0.055669	4.733379
273.969606	7713.267011	14.425984	-0.055638	4.730969
274.185324	7705.319218	14.430989	-0.055673	4.728603
273.860336	7697.303347	14.435994	-0.055607	4.726218
274.008699	7689.317851	14.440999	-0.055629	4.723838
274.224950	7681.359958	14.446003	-0.055664	4.721466
273.869203	7673.292291	14.451008	-0.055592	4.719061
273.751198	7665.354294	14.456013	-0.055565	4.716693
273.801450	7657.323410	14.461018	-0.055569	4.714296
273.706600	7649.244247	14.466023	-0.055546	4.711883
273.773608	7641.306304	14.471027	-0.055553	4.709511
273.739988	7633.285979	14.476032	-0.055542	4.707113
273.951998	7625.281992	14.481037	-0.055576	4.704719
273.808507	7617.357700	14.486042	-0.055544	4.702347
273.532748	7609.281233	14.491047	-0.055487	4.699930
273.576595	7601.373720	14.496051	-0.055490	4.697561
273.528272	7593.280059	14.501056	-0.055475	4.695135
273.613252	7585.319474	14.506061	-0.055486	4.692748
273.625267	7577.269882	14.511066	-0.055483	4.690332
273.625836	7569.242049	14.516071	-0.055477	4.687923
273.468019	7561.278753	14.521075	-0.055443	4.685531
273.332272	7553.312445	14.526080	-0.055412	4.683137
273.367479	7545.290976	14.531085	-0.055413	4.680726
273.289830	7537.312481	14.536090	-0.055393	4.678326
273.344005	7529.328406	14.541095	-0.055398	4.675923
273.407745	7521.238596	14.546099	-0.055405	4.673487
273.302049	7513.152211	14.551104	-0.055380	4.671051
273.313167	7505.216605	14.556109	-0.055376	4.668658
273.322854	7497.203307	14.561114	-0.055373	4.666242
273.294944	7489.190912	14.566119	-0.055362	4.663824
273.289946	7481.278925	14.571123	-0.055356	4.661435
273.054443	7473.243072	14.576128	-0.055307	4.659008
273.173626	7465.256100	14.581133	-0.055324	4.656594
273.116670	7457.196277	14.586138	-0.055308	4.654157
273.035388	7449.230388	14.591143	-0.055287	4.651748
272.950630	7441.209883	14.596147	-0.055266	4.649320
272.794240	7433.212999	14.601152	-0.055231	4.646898
272.587474	7425.170788	14.606157	-0.055188	4.644461
272.753303	7417.269626	14.611162	-0.055213	4.642066
272.909869	7409.223265	14.616167	-0.055237	4.639625
272.801616	7401.276234	14.621171	-0.055211	4.637213
272.540055	7393.207725	14.626176	-0.055157	4.634764
272.803019	7385.189579	14.631181	-0.055201	4.632327
272.766479	7377.187491	14.636186	-0.055189	4.629895
272.627407	7369.190544	14.641191	-0.055158	4.627463
272.675536	7361.189828	14.646195	-0.055161	4.625029
272.831810	7353.211847	14.651200	-0.055185	4.622600
272.533931	7345.145550	14.656205	-0.055124	4.620143
272.461103	7337.234285	14.661210	-0.055105	4.617731
272.320428	7329.171599	14.666215	-0.055074	4.615273
272.270096	7321.165441	14.671219	-0.055059	4.612830
272.230481	7313.128785	14.676224	-0.055046	4.610377
272.168685	7305.149581	14.681229	-0.055029	4.607940
272.304650	7297.203103	14.686234	-0.055049	4.605512
272.022173	7289.204974	14.691239	-0.054991	4.603066
272.091445	7281.203711	14.696243	-0.054999	4.600619
272.184073	7273.191363	14.701248	-0.055011	4.598166
272.088452	7265.152953	14.706253	-0.054988	4.595704
272.081047	7257.150332	14.711258	-0.054981	4.593252
272.179400	7249.059158	14.716263	-0.054994	4.590772
272.171001	7241.138402	14.721267	-0.054987	4.588342
272.026178	7233.115365	14.726272	-0.054954	4.585880
272.009466	7225.114694	14.731277	-0.054946	4.583423
272.212419	7217.146207	14.736282	-0.054978	4.580975
272.083098	7209.117845	14.741287	-0.054949	4.578508
272.139163	7201.140005	14.746291	-0.054954	4.576054
271.936331	7193.133775	14.751296	-0.054911	4.573590
271.897411	7185.070575	14.756301	-0.054898	4.571107
271.852002	7177.147568	14.761306	-0.054885	4.568667
271.859473	7169.116221	14.766311	-0.054881	4.566191
271.934109	7161.124394	14.771315	-0.054889	4.563727
271.692307	7153.121984	14.776320	-0.054839	4.561257
271.721602	7145.127895	14.781325	-0.054839	4.558789
271.848224	7137.186195	14.786330	-0.054857	4.556336
271.693446	7129.110689	14.791335	-0.054823	4.553840
271.562099	7121.084986	14.796339	-0.054793	4.551358
271.554428	7113.083267	14.801344	-0.054786	4.548883
271.546471	7105.073818	14.806349	-0.054779	4.546403
271.491443	7097.114353	14.811354	-0.054764	4.543938
271.566014	7089.126275	14.816359	-0.054772	4.541462
271.575697	7081.091578	14.821363	-0.054769	4.538971
271.421838	7073.157859	14.826368	-0.054735	4.536509
271.387527	7065.072926	14.831373	-0.054723	4.533999
271.407751	7057.110720	14.836378	-0.054721	4.531526
271.142569	7049.066373	14.841383	-0.054667	4.529026
271.061207	7041.130722	14.846387	-0.054646	4.526558
271.099074	7033.120348	14.851392	-0.054648	4.524066
271.271281	7025.148506	14.856397	-0.054675	4.521585
271.307856	7017.117849	14.861402	-0.054676	4.519084
271.138027	7009.121247	14.866407	-0.054639	4.516592
271.198710	7001.081287	14.871411	-0.054645	4.514085
271.167265	6992.993491	14.876416	-0.054634	4.511562
271.025910	6985.005132	14.881421	-0.054602	4.509068
271.185854	6977.056706	14.886426	-0.054627	4.506586
270.931553	6969.017276	14.891431	-0.054574	4.504073
270.881310	6961.090459	14.896435	-0.054559	4.501595
270.862150	6953.062998	14.901440	-0.054550	4.499083
270.953197	6945.090878	14.906445	-0.054562	4.496588
270.790643	6937.028859	14.911450	-0.054526	4.494063
270.699514	6929.039487	14.916455	-0.054504	4.491559
270.874169	6921.042072	14.921459	-0.054531	4.489052
270.877958	6913.059715	14.926464	-0.054526	4.486548
270.774181	6905.031206	14.931469	-0.054502	4.484028
270.762304	6897.093764	14.936474	-0.054494	4.481535
270.707761	6889.033075	14.941479	-0.054479	4.479002
270.610740	6881.095557	14.946483	-0.054455	4.476505
270.571957	6873.045802	14.951488	-0.054443	4.473973
270.525874	6864.985837	14.956493	-0.054429	4.471436
270.503368	6856.993630	14.961498	-0.054419	4.468918
270.501767	6849.001742	14.966503	-0.054413	4.466400
270.589925	6841.053906	14.971507	-0.054425	4.463894
270.276067	6833.032178	14.976512	-0.054361	4.461362
270.303262	6825.099018	14.981517	-0.054360	4.458858
270.420720	6817.073354	14.986522	-0.054377	4.456324
270.218186	6808.996946	14.991527	-0.054334	4.453770
270.184274	6800.947802	14.996531	-0.054322	4.451225
270.113606	6792.980700	15.001536	-0.054304	4.448704
270.182527	6784.960134	15.006541	-0.054311	4.446165
270.150957	6777.035127	15.011546	-0.054300	4.443655
269.865026	6769.005767	15.016551	-0.054241	4.441109
269.991596	6761.041459	15.021555	-0.054260	4.438584
269.901140	6753.024636	15.026560	-0.054237	4.436040
269.924817	6744.958754	15.031565	-0.054236	4.433479
269.874948	6736.947702	15.036570	-0.054222	4.430934
269.795235	6728.937782	15.041575	-0.054202	4.428388
269.740255	6720.904670	15.046579	-0.054186	4.425833
269.809447	6712.948934	15.051584	-0.054193	4.423301
269.783343	6704.966812	15.056589	-0.054183	4.420760
269.789687	6697.032892	15.061594	-0.054179	4.418232
269.817825	6688.965128	15.066599	-0.054179	4.415660
269.922781	6680.986000	15.071603	-0.054193	4.413116
269.700870	6672.944216	15.076608	-0.054146	4.410548
269.586587	6664.953389	15.081613	-0.054120	4.407996
269.770931	6656.972195	15.086618	-0.054149	4.405447
269.727751	6648.988531	15.091623	-0.054135	4.402895
269.550378	6640.991250	15.096627	-0.054097	4.400335
269.390444	6633.004258	15.101632	-0.054062	4.397778
269.289735	6624.975179	15.106637	-0.054038	4.395206
269.415707	6616.986905	15.111642	-0.054056	4.392647
269.196240	6608.920637	15.116647	-0.054010	4.390060
269.474444	6600.889431	15.121651	-0.054056	4.387485
269.402372	6592.889450	15.126656	-0.054037	4.384916
269.432717	6584.984674	15.131661	-0.054038	4.382377
269.520484	6576.991179	15.136666	-0.054049	4.379809
269.437441	6569.079229	15.141671	-0.054028	4.377264
269.403467	6560.995445	15.146675	-0.054016	4.374663
269.191189	6552.985737	15.151680	-0.053971	4.372083
269.060626	6544.923118	15.156685	-0.053942	4.369485
269.296070	6537.035580	15.161690	-0.053980	4.366944
268.982096	6528.949251	15.166695	-0.053916	4.364334
268.903985	6521.013214	15.171699	-0.053896	4.361772
269.018628	6512.983376	15.176704	-0.053912	4.359180
268.874766	6505.007833	15.181709	-0.053880	4.356602
268.943950	6496.934344	15.186714	-0.053888	4.353992
268.895975	6488.823661	15.191719	-0.053873	4.351368
268.915405	6480.886229	15.196723	-0.053872	4.348799
268.928368	6472.932420	15.201728	-0.053869	4.346223
268.680820	6464.917474	15.206733	-0.053817	4.343624
268.696743	6456.971208	15.211738	-0.053815	4.341048
268.587145	6448.959211	15.216743	-0.053789	4.338447
268.727003	6440.970775	15.221747	-0.053810	4.335855
268.789072	6432.924374	15.226752	-0.053816	4.333241
268.688270	6424.921880	15.231757	-0.053792	4.330640
268.477361	6416.947771	15.236762	-0.053747	4.328045
268.433469	6408.927848	15.241767	-0.053734	4.325434
268.617439	6400.978631	15.246771	-0.053763	4.322847
268.408710	6392.973025	15.251776	-0.053718	4.320237
268.421475	6384.971147	15.256781	-0.053715	4.317628
268.553003	6376.967561	15.261786	-0.053735	4.315018
268.436281	6368.887499	15.266791	-0.053707	4.312380
268.427515	6360.884456	15.271795	-0.053700	4.309766
268.459333	6352.933075	15.276800	-0.053701	4.307167
268.434243	6344.885716	15.281805	-0.053691	4.304536
268.370729	6336.948179	15.286810	-0.053674	4.301938
268.404548	6328.889208	15.291815	-0.053675	4.299299
268.227785	6320.942221	15.296819	-0.053637	4.296694
268.149890	6312.936783	15.301824	-0.053617	4.294069
268.106164	6304.854561	15.306829	-0.053603	4.291418
268.336429	6296.912236	15.311834	-0.053641	4.288813
268.160251	6288.895499	15.316839	-0.053602	4.286178
268.067631	6280.920600	15.321843	-0.053580	4.283557
268.105248	6272.966300	15.326848	-0.053582	4.280942
268.010003	6264.925402	15.331853	-0.053558	4.278295
267.983442	6256.954111	15.336858	-0.053548	4.275670
267.860081	6248.854776	15.341863	-0.053520	4.273001
267.954606	6240.854264	15.346867	-0.053532	4.270365
267.854940	6232.871358	15.351872	-0.053508	4.267731
267.836337	6224.834536	15.356877	-0.053499	4.265078
267.932464	6216.922511	15.361882	-0.053512	4.262466
267.655299	6208.844042	15.366887	-0.053455	4.259794
267.586010	6200.924625	15.371891	-0.053437	4.257174
267.764986	6192.882587	15.376896	-0.053465	4.254515
267.652690	6184.885589	15.381901	-0.053438	4.251866
267.693075	6176.844172	15.386906	-0.053440	4.249202
267.645822	6168.901563	15.391911	-0.053426	4.246569
267.567285	6160.884811	15.396915	-0.053406	4.243909
267.526996	6152.943504	15.401920	-0.053394	4.241273
267.493948	6144.916740	15.406925	-0.053382	4.238607
267.690645	6136.969216	15.411930	-0.053413	4.235967
267.466312	6128.870746	15.416935	-0.053366	4.233272
267.339766	6120.873171	15.421939	-0.053337	4.230610
267.529552	6112.916415	15.426944	-0.053367	4.227962
267.375377	6104.870737	15.431949	-0.053333	4.225280
267.307513	6096.940952	15.436954	-0.053315	4.222636
267.152854	6088.906494	15.441959	-0.053281	4.219954
267.204006	6080.962653	15.446963	-0.053285	4.217303
267.396079	6072.928895	15.451968	-0.053316	4.214621
267.095432	6064.904914	15.456973	-0.053254	4.211936
267.319860	6056.885951	15.461978	-0.053291	4.209257
267.125898	6048.905433	15.466983	-0.053249	4.206584
267.078408	6040.918071	15.471987	-0.053235	4.203909
267.045449	6032.926054	15.476992	-0.053224	4.201230
266.907683	6024.952686	15.481997	-0.053193	4.198555
266.900757	6016.910562	15.487002	-0.053186	4.195857
266.850372	6008.784833	15.492007	-0.053171	4.193128
266.979555	6000.777586	15.497011	-0.053190	4.190440
266.923037	5992.862185	15.502016	-0.053174	4.187778
266.717831	5984.845325	15.507021	-0.053130	4.185079
266.850581	5976.882057	15.512026	-0.053150	4.182400
266.644749	5968.879347	15.517031	-0.053106	4.179703
266.678483	5960.897147	15.522035	-0.053107	4.177013
266.737370	5952.891486	15.527040	-0.053113	4.174313
266.556129	5944.891600	15.532045	-0.053073	4.171612
266.501389	5936.872401	15.537050	-0.053058	4.168903
266.563389	5928.875747	15.542055	-0.053064	4.166201
266.391993	5920.884801	15.547059	-0.053027	4.163498
266.477269	5912.892207	15.552064	-0.053037	4.160794
266.304804	5904.892427	15.557069	-0.053000	4.158084
266.442330	5896.926851	15.562074	-0.053020	4.155387
266.310093	5888.810977	15.567079	-0.052990	4.152634
266.283924	5880.817363	15.572083	-0.052980	4.149921
266.452407	5872.861693	15.577088	-0.053006	4.147223
266.311959	5864.816384	15.582093	-0.052974	4.144488
266.255504	5856.913034	15.587098	-0.052959	4.141801
266.229624	5848.874279	15.592103	-0.052948	4.139067
266.265492	5840.873485	15.597107	-0.052950	4.136344
266.014424	5832.891052	15.602112	-0.052898	4.133622
265.810919	5824.860064	15.607117	-0.052854	4.130883
265.846679	5816.875190	15.612122	-0.052856	4.128160
265.899106	5808.829119	15.617127	-0.052860	4.125415
265.887939	5800.875729	15.622131	-0.052853	4.122699
265.753624	5792.881921	15.627136	-0.052822	4.119965
265.906916	5784.902852	15.632141	-0.052845	4.117239
265.866817	5776.862370	15.637146	-0.052833	4.114487
265.583117	5768.771741	15.642151	-0.052774	4.111713
265.757323	5760.857932	15.647155	-0.052802	4.109004
265.742570	5752.873625	15.652160	-0.052793	4.106266
265.575870	5744.858617	15.657165	-0.052757	4.103514
265.677202	5736.904223	15.662170	-0.052771	4.100785
265.603023	5728.900090	15.667175	-0.052751	4.098034
265.508582	5720.891260	15.672179	-0.052728	4.095279
265.513809	5712.894869	15.677184	-0.052724	4.092528
265.341654	5704.836465	15.682189	-0.052687	4.089752
265.342843	5696.923560	15.687194	-0.052682	4.087026
265.277539	5688.831157	15.692199	-0.052664	4.084236
265.248668	5680.921109	15.697203	-0.052653	4.081507
265.271701	5672.912128	15.702208	-0.052652	4.078743
264.988360	5664.936231	15.707213	-0.052594	4.075984
265.210264	5656.927425	15.712218	-0.052630	4.073219
265.274250	5648.879843	15.717223	-0.052637	4.070436
265.066993	5640.910104	15.722227	-0.052593	4.067675
265.128305	5632.885325	15.727232	-0.052599	4.064896
265.316156	5624.897732	15.732237	-0.052628	4.062130
265.282842	5616.924643	15.737242	-0.052617	4.059364
264.987925	5608.932793	15.742247	-0.052557	4.056586
265.146905	5600.862927	15.747251	-0.052581	4.053786
265.166293	5592.892429	15.752256	-0.052579	4.051016
264.980477	5584.882171	15.757261	-0.052539	4.048228
265.182694	5576.906853	15.762266	-0.052571	4.045455
264.979924	5568.935302	15.767271	-0.052528	4.042676
264.871094	5560.913377	15.772275	-0.052503	4.039878
264.957185	5552.964777	15.777280	-0.052513	4.037108
265.033563	5544.886987	15.782285	-0.052522	4.034290
264.940965	5536.815867	15.787290	-0.052500	4.031470
264.762273	5528.821156	15.792295	-0.052461	4.028673
264.886409	5520.856351	15.797299	-0.052479	4.025889
264.845121	5512.893556	15.802304	-0.052466	4.023102
264.669048	5504.869160	15.807309	-0.052427	4.020289
264.685658	5496.951482	15.812314	-0.052425	4.017515
264.815185	5488.875855	15.817319	-0.052444	4.014684
264.751484	5480.842059	15.822323	-0.052427	4.011864
264.646546	5472.883332	15.827328	-0.052402	4.009067
264.537534	5464.883326	15.832333	-0.052376	4.006254
264.639784	5456.921160	15.837338	-0.052390	4.003456
264.433962	5448.908444	15.842343	-0.052346	4.000632
264.435417	5440.941660	15.847347	-0.052341	3.997827
264.512943	5432.917665	15.852352	-0.052350	3.995000
264.465650	5424.836920	15.857357	-0.052336	3.992149
264.502254	5416.880135	15.862362	-0.052338	3.989342
264.327151	5408.870709	15.867367	-0.052300	3.986510
264.318682	5400.887560	15.872371	-0.052293	3.983688
264.176079	5392.918991	15.877376	-0.052261	3.980868
264.333535	5384.895329	15.882381	-0.052285	3.978030
264.188657	5376.932986	15.887386	-0.052252	3.975208
264.062843	5368.890936	15.892391	-0.052224	3.972355
264.149797	5360.860458	15.897395	-0.052234	3.969508
264.129371	5352.925238	15.902400	-0.052225	3.966691
263.899806	5344.914309	15.907405	-0.052177	3.963842
263.937180	5336.917483	15.912410	-0.052179	3.961000
263.965114	5328.900524	15.917415	-0.052179	3.958148
263.888202	5320.943514	15.922419	-0.052159	3.955315
263.769152	5312.922457	15.927424	-0.052131	3.952455
263.890786	5304.893756	15.932429	-0.052149	3.949595
264.025852	5296.949776	15.937434	-0.052169	3.946763
263.606763	5288.918092	15.942439	-0.052085	3.943889
263.749642	5280.957268	15.947443	-0.052106	3.941047
263.763302	5272.969264	15.952448	-0.052104	3.938191
263.725899	5264.944241	15.957453	-0.052091	3.935319
263.599889	5256.950450	15.962458	-0.052062	3.932455
263.494529	5248.895311	15.967463	-0.052037	3.929567
263.629450	5240.925426	15.972467	-0.052057	3.926711
263.565932	5232.951322	15.977472	-0.052040	3.923849
263.491624	5224.976666	15.982477	-0.052021	3.920984
263.545781	5216.967461	15.987482	-0.052026	3.918107
263.372888	5208.985286	15.992487	-0.051988	3.915233
263.273239	5200.960199	15.997491	-0.051964	3.912343
263.436481	5192.967398	16.002496	-0.051989	3.909467
263.387434	5184.938582	16.007501	-0.051975	3.906572
263.232061	5176.995678	16.012506	-0.051940	3.903704
263.387379	5168.946517	16.017511	-0.051964	3.900802
263.308765	5160.974278	16.022515	-0.051944	3.897921
263.073336	5152.977360	16.027520	-0.051895	3.895025
263.117777	5144.945002	16.032525	-0.051898	3.892120
263.245326	5136.925437	16.037530	-0.051916	3.889219
263.140557	5128.948264	16.042535	-0.051891	3.886327
262.875143	5120.955516	16.047539	-0.051836	3.883424
263.107788	5112.998992	16.052544	-0.051874	3.880541
262.947541	5105.004060	16.057549	-0.051839	3.877635
263.000125	5096.950487	16.062554	-0.051844	3.874709
262.948674	5088.702654	16.067559	-0.051829	3.871709
263.075865	5080.800542	16.072563	-0.051847	3.868835
262.911801	5072.878129	16.077568	-0.051811	3.865947
262.792009	5064.896792	16.082573	-0.051783	3.863035
262.957761	5056.928116	16.087578	-0.051809	3.860132
262.789387	5048.957258	16.092583	-0.051772	3.857218
262.503797	5040.950281	16.097587	-0.051714	3.854287
262.609213	5032.959438	16.102592	-0.051728	3.851368
262.537721	5024.943513	16.107597	-0.051709	3.848434
262.489962	5016.957983	16.112602	-0.051695	3.845509
262.465225	5009.004521	16.117607	-0.051685	3.842594
262.357481	5000.979229	16.122611	-0.051660	3.839648
262.421581	4993.033792	16.127616	-0.051666	3.836734
262.321750	4984.993187	16.132621	-0.051642	3.833778
262.441689	4976.984561	16.137626	-0.051659	3.830837
262.326818	4968.997115	16.142631	-0.051633	3.827897
262.206658	4960.963606	16.147635	-0.051605	3.824937
262.374426	4953.040145	16.152640	-0.051631	3.822021
262.182258	4945.040961	16.157645	-0.051590	3.819068
262.216699	4937.058651	16.162650	-0.051591	3.816123
262.220171	4929.047103	16.167655	-0.051586	3.813164
262.150530	4921.003806	16.172659	-0.051568	3.810190
262.109316	4913.072330	16.177664	-0.051555	3.807256
261.854929	4905.005173	16.182669	-0.051502	3.804265
262.001040	4897.071769	16.187674	-0.051524	3.801329
262.023422	4889.061649	16.192679	-0.051523	3.798360
261.960664	4881.057774	16.197683	-0.051506	3.795389
261.994996	4873.039314	16.202688	-0.051507	3.792413
261.861940	4865.015263	16.207693	-0.051476	3.789428
261.911687	4857.046271	16.212698	-0.051480	3.786465
261.746335	4849.042713	16.217703	-0.051444	3.783483
261.820079	4841.043752	16.222707	-0.051453	3.780505
261.668008	4833.085604	16.227712	-0.051419	3.777535
261.513635	4825.021832	16.232717	-0.051385	3.774523
261.597034	4817.078874	16.237722	-0.051395	3.771560
261.713843	4809.036532	16.242727	-0.051411	3.768557
261.606469	4801.047618	16.247731	-0.051386	3.765567
261.647393	4793.076870	16.252736	-0.051388	3.762585
261.667667	4785.047876	16.257741	-0.051387	3.759578
261.727542	4777.119438	16.262746	-0.051393	3.756608
261.709210	4769.072311	16.267751	-0.051384	3.753589
261.376044	4761.087766	16.272755	-0.051316	3.750583
261.243505	4753.155434	16.277760	-0.051286	3.747599
261.145957	4745.046390	16.282765	-0.051263	3.744548
261.134506	4737.106943	16.287770	-0.051255	3.741559
261.095797	4729.103481	16.292775	-0.051243	3.738544
260.946722	4721.112620	16.297779	-0.051210	3.735528
260.945198	4713.128892	16.302784	-0.051204	3.732516
260.992941	4705.028651	16.307789	-0.051207	3.729458
261.002515	4697.107586	16.312794	-0.051204	3.726465
260.816558	4689.122832	16.317799	-0.051164	3.723441
260.859475	4681.121776	16.322803	-0.051167	3.720413
260.982945	4673.167366	16.327808	-0.051184	3.717403
260.785303	4665.152750	16.332813	-0.051142	3.714360
260.718604	4657.062327	16.337818	-0.051124	3.711289
260.685674	4649.061918	16.342823	-0.051113	3.708250
260.784678	4641.084159	16.347827	-0.051126	3.705220
260.814725	4633.129684	16.352832	-0.051126	3.702195
260.576550	4625.131173	16.357837	-0.051076	3.699144
260.463941	4617.193402	16.362842	-0.051050	3.696117
260.613949	4609.134456	16.367847	-0.051073	3.693048
260.527914	4601.134495	16.372851	-0.051051	3.689993
260.557163	4593.183429	16.377856	-0.051051	3.686957
260.478604	4585.195433	16.382861	-0.051031	3.683901
260.600588	4577.208938	16.387866	-0.051049	3.680849
260.467360	4569.219131	16.392871	-0.051019	3.677786
260.352676	4561.193273	16.397875	-0.050992	3.674707
260.467277	4553.160459	16.402880	-0.051008	3.671629
260.511047	4545.139910	16.407885	-0.051011	3.668552
260.413722	4537.184328	16.412890	-0.050987	3.665493
260.113224	4529.252418	16.417895	-0.050926	3.662435
260.200511	4521.186640	16.422899	-0.050937	3.659333
260.183366	4513.249822	16.427904	-0.050928	3.656276
260.007413	4505.191242	16.432909	-0.050890	3.653165
260.073418	4497.157847	16.437914	-0.050897	3.650067
259.945368	4489.215675	16.442919	-0.050868	3.646997
260.004622	4481.187433	16.447923	-0.050874	3.643896
259.870217	4473.256812	16.452928	-0.050843	3.640825
259.877011	4465.239348	16.457933	-0.050839	3.637721
259.976879	4457.231940	16.462938	-0.050852	3.634621
259.811603	4449.221597	16.467943	-0.050816	3.631511
259.720824	4441.192098	16.472947	-0.050794	3.628392
259.838653	4433.217624	16.477952	-0.050811	3.625297
259.834111	4425.227992	16.482957	-0.050804	3.622191
259.883721	4417.245424	16.487962	-0.050808	3.619086
259.795025	4409.294667	16.492967	-0.050786	3.615987
259.655730	4401.279091	16.497971	-0.050755	3.612859
259.525913	4393.257857	16.502976	-0.050726	3.609726
259.558914	4385.275233	16.507981	-0.050726	3.606610
259.539383	4377.271304	16.512986	-0.050717	3.603481
259.481712	4369.296214	16.517991	-0.050701	3.600360
259.404961	4361.323062	16.522995	-0.050682	3.597237
259.537617	4353.311564	16.528000	-0.050701	3.594101
259.412611	4345.308062	16.533005	-0.050672	3.590959
259.145874	4337.356054	16.538010	-0.050617	3.587830
259.304078	4329.350936	16.543015	-0.050641	3.584690
259.141472	4321.356228	16.548019	-0.050606	3.581542
259.106116	4313.375220	16.553024	-0.050594	3.578400
259.124589	4305.359286	16.558029	-0.050592	3.575243
259.284874	4297.358253	16.563034	-0.050617	3.572093
259.175682	4289.319934	16.568039	-0.050591	3.568918
259.040783	4281.380791	16.573043	-0.050560	3.565778
259.164210	4273.386225	16.578048	-0.050578	3.562622
258.969395	4265.387536	16.583053	-0.050536	3.559451
258.976103	4257.424461	16.588058	-0.050532	3.556298
258.937570	4249.318287	16.593063	-0.050520	3.553084
258.856931	4241.250930	16.598067	-0.050499	3.549881
258.791862	4233.361058	16.603072	-0.050482	3.546746
258.629401	4225.332382	16.608077	-0.050446	3.543550
258.766722	4217.380286	16.613082	-0.050466	3.540391
258.779105	4209.412508	16.618087	-0.050463	3.537219
258.607962	4201.379601	16.623091	-0.050426	3.534013
258.788617	4193.397059	16.628096	-0.050454	3.530835
258.569167	4185.385562	16.633101	-0.050408	3.527630
258.486011	4177.408564	16.638106	-0.050387	3.524439
258.654074	4169.438389	16.643111	-0.050413	3.521257
258.448199	4161.433016	16.648115	-0.050370	3.518046
258.465433	4153.471680	16.653120	-0.050368	3.514856
258.444206	4145.428708	16.658125	-0.050358	3.511630
258.515093	4137.422580	16.663130	-0.050366	3.508419
258.363316	4129.447952	16.668135	-0.050332	3.505210
258.251359	4121.451235	16.673139	-0.050306	3.501990
258.333577	4113.508868	16.678144	-0.050316	3.498796
258.329798	4105.480502	16.683149	-0.050310	3.495561
258.301636	4097.480050	16.688154	-0.050300	3.492334
258.225751	4089.499249	16.693159	-0.050280	3.489110
258.052024	4081.515773	16.698163	-0.050242	3.485879
258.068844	4073.560300	16.703168	-0.050240	3.482663
257.839567	4065.549850	16.708173	-0.050192	3.479413
258.049926	4057.568486	16.713178	-0.050226	3.476186
258.101775	4049.515424	16.718183	-0.050230	3.472922
257.957344	4041.500106	16.723187	-0.050198	3.469664
257.928557	4033.536181	16.728192	-0.050187	3.466427
257.842997	4025.535132	16.733197	-0.050166	3.463171
257.844052	4017.547759	16.738202	-0.050161	3.459920
257.626807	4009.550169	16.743207	-0.050115	3.456654
257.814718	4001.515440	16.748211	-0.050145	3.453383
257.949023	3993.556773	16.753216	-0.050164	3.450139
257.759099	3985.604987	16.758221	-0.050124	3.446884
257.798606	3977.612478	16.763226	-0.050126	3.443616
257.875260	3969.620716	16.768231	-0.050135	3.440347
257.914170	3961.611412	16.773235	-0.050136	3.437066
257.943991	3953.624179	16.778240	-0.050137	3.433791
257.639249	3945.602727	16.783245	-0.050075	3.430488
257.749874	3937.635619	16.788250	-0.050090	3.427218
257.800616	3929.599054	16.793255	-0.050094	3.423914
257.623724	3921.651866	16.798259	-0.050056	3.420636
257.402500	3913.713012	16.803264	-0.050009	3.417356
257.372013	3905.680638	16.808269	-0.049998	3.414042
257.625137	3897.637115	16.813274	-0.050040	3.410729
257.581281	3889.681830	16.818279	-0.050026	3.407439
257.313816	3881.698567	16.823283	-0.049971	3.404127
257.302200	3873.738773	16.828288	-0.049964	3.400830
257.548614	3865.718453	16.833293	-0.050004	3.397514
257.357750	3857.743267	16.838298	-0.049963	3.394198
257.301937	3849.656435	16.843303	-0.049948	3.390837
257.261606	3841.667163	16.848307	-0.049935	3.387514
257.207393	3833.692175	16.853312	-0.049919	3.384193
257.028149	3825.743116	16.858317	-0.049881	3.380876
256.893377	3817.774979	16.863322	-0.049850	3.377548
257.087145	3809.765904	16.868327	-0.049881	3.374212
256.863778	3801.750909	16.873331	-0.049834	3.370855
256.917933	3793.794921	16.878336	-0.049839	3.367530
256.877528	3785.766912	16.883341	-0.049826	3.364167
256.842482	3777.802339	16.888346	-0.049814	3.360828
256.809089	3769.821756	16.893351	-0.049802	3.357479
256.823127	3761.800483	16.898355	-0.049800	3.354112
256.861325	3753.777753	16.903360	-0.049801	3.350741
256.696667	3745.815497	16.908365	-0.049765	3.347385
256.827938	3737.803041	16.913370	-0.049784	3.344015
256.820278	3729.858051	16.918375	-0.049778	3.340665
256.706068	3721.868952	16.923379	-0.049751	3.337289
256.529459	3713.877932	16.928384	-0.049713	3.333907
256.487763	3705.859692	16.933389	-0.049700	3.330514
256.516678	3697.876624	16.938394	-0.049700	3.327136
256.488038	3689.915551	16.943399	-0.049689	3.323761
256.499069	3681.900236	16.948403	-0.049686	3.320362
256.485217	3673.957791	16.953408	-0.049678	3.316989
256.360320	3665.923141	16.958413	-0.049649	3.313569
256.254500	3657.894425	16.963418	-0.049624	3.310149
256.343024	3649.909540	16.968423	-0.049635	3.306751
256.233644	3641.917515	16.973427	-0.049610	3.303340
256.094426	3633.977409	16.978432	-0.049578	3.299945
256.146389	3625.996307	16.983437	-0.049583	3.296537
256.081373	3617.993797	16.988442	-0.049565	3.293112
256.123748	3609.975425	16.993447	-0.049568	3.289681
255.991611	3602.002955	16.998451	-0.049538	3.286259
256.079503	3594.026281	17.003456	-0.049549	3.282840
255.948585	3586.020263	17.008461	-0.049519	3.279396
255.939026	3578.086482	17.013466	-0.049512	3.275985
256.034283	3570.049230	17.018471	-0.049524	3.272529
255.879399	3562.026527	17.023475	-0.049490	3.269067
255.886315	3554.056252	17.028480	-0.049486	3.265629
255.781808	3546.079256	17.033485	-0.049461	3.262181
255.842898	3538.080425	17.038490	-0.049467	3.258726
255.591147	3530.113709	17.043495	-0.049415	3.255269
255.438876	3522.062868	17.048499	-0.049381	3.251776
255.563126	3514.095303	17.053504	-0.049399	3.248326
255.540313	3506.093655	17.058509	-0.049389	3.244852
255.483385	3498.160479	17.063514	-0.049374	3.241403
255.584617	3490.182377	17.068519	-0.049387	3.237936
255.523961	3482.146845	17.073523	-0.049370	3.234435
255.446532	3474.113021	17.078528	-0.049351	3.230929
255.460563	3466.123754	17.083533	-0.049348	3.227443
255.523461	3458.124976	17.088538	-0.049354	3.223951
255.489433	3450.176025	17.093543	-0.049343	3.220473
255.248374	3442.200954	17.098547	-0.049292	3.216972
255.477190	3434.208281	17.103552	-0.049330	3.213478
255.523595	3426.175965	17.108557	-0.049333	3.209955
255.005272	3418.247705	17.113562	-0.049231	3.206451
255.175919	3410.280181	17.118567	-0.049257	3.202955
255.077127	3402.264616	17.123571	-0.049234	3.199422
255.013709	3394.321855	17.128576	-0.049217	3.195919
254.945608	3386.287858	17.133581	-0.049199	3.192371
254.988113	3378.276999	17.138586	-0.049201	3.188834
255.158578	3370.301584	17.143591	-0.049227	3.185315
254.907871	3362.335786	17.148595	-0.049175	3.181778
254.928449	3354.362080	17.153600	-0.049174	3.178245
254.848726	3346.340070	17.158605	-0.049154	3.174683
254.727178	3338.366264	17.163610	-0.049126	3.171136
254.829787	3330.384002	17.168615	-0.049140	3.167591
254.712773	3322.357586	17.173619	-0.049112	3.164013
254.685970	3314.425381	17.178624	-0.049102	3.160476
254.542736	3306.457436	17.183629	-0.049070	3.156915
254.757952	3298.391008	17.188634	-0.049105	3.153321
254.687164	3290.420883	17.193639	-0.049086	3.149754
254.484239	3282.426045	17.198643	-0.049043	3.146166
254.584769	3274.461531	17.203648	-0.049056	3.142601
254.280722	3266.473392	17.208653	-0.048995	3.139003
254.418380	3258.469889	17.213658	-0.049015	3.135414
254.542859	3250.489272	17.218663	-0.049033	3.131830
254.262704	3242.516094	17.223667	-0.048975	3.128227
254.193197	3234.516875	17.228672	-0.048957	3.124618
254.048611	3226.583463	17.233677	-0.048925	3.121031
254.252242	3218.578403	17.238682	-0.048957	3.117424
254.214124	3210.607941	17.243687	-0.048945	3.113816
254.022231	3202.567675	17.248691	-0.048904	3.110167
254.215768	3194.594797	17.253696	-0.048934	3.106560
254.117299	3186.606688	17.258701	-0.048911	3.102930
254.018977	3178.643757	17.263706	-0.048887	3.099306
254.099943	3170.670123	17.268711	-0.048897	3.095682
254.103495	3162.635497	17.273715	-0.048892	3.092022
254.099138	3154.660440	17.278720	-0.048886	3.088385
253.916459	3146.674533	17.283725	-0.048846	3.084730
253.975482	3138.720132	17.288730	-0.048852	3.081096
253.878469	3130.750009	17.293735	-0.048829	3.077444
253.700368	3122.736359	17.298739	-0.048790	3.073763
253.825951	3114.664761	17.303744	-0.048808	3.070066
253.592896	3106.708010	17.308749	-0.048759	3.066400
253.562905	3098.743536	17.313754	-0.048749	3.062735
253.519808	3090.788598	17.318759	-0.048735	3.059071
253.442214	3082.802087	17.323763	-0.048715	3.055385
253.387991	3074.822176	17.328768	-0.048700	3.051699
253.397633	3066.814303	17.333773	-0.048696	3.047999
253.217440	3058.837083	17.338778	-0.048658	3.044299
253.500491	3050.858150	17.343783	-0.048705	3.040617
253.340960	3042.890840	17.348787	-0.048670	3.036914
253.302688	3034.904628	17.353792	-0.048657	3.033203
253.480189	3026.864851	17.358797	-0.048685	3.029474
253.176975	3018.923141	17.363802	-0.048623	3.025762
253.191203	3010.937469	17.368807	-0.048621	3.022040
253.114235	3002.959124	17.373811	-0.048601	3.018313
253.171928	2994.965225	17.378816	-0.048606	3.014581
252.969311	2986.972490	17.383821	-0.048563	3.010832
252.987801	2978.966582	17.388826	-0.048561	3.007083
252.968765	2971.015847	17.393831	-0.048552	3.003353
252.892131	2963.031909	17.398835	-0.048533	2.999600
252.945619	2955.086725	17.403840	-0.048537	2.995867
252.827666	2947.044304	17.408845	-0.048510	2.992075
252.693758	2939.061492	17.413850	-0.048480	2.988305
252.691045	2931.072903	17.418855	-0.048474	2.984535
252.995739	2923.070936	17.423859	-0.048525	2.980769
252.729160	2915.156325	17.428864	-0.048470	2.977011
252.533184	2907.167253	17.433869	-0.048429	2.973216
252.505380	2899.146810	17.438874	-0.048418	2.969410
252.668270	2891.164833	17.443879	-0.048443	2.965627
252.461087	2883.211709	17.448883	-0.048399	2.961834
252.351249	2875.268237	17.453888	-0.048373	2.958046
252.262302	2867.254224	17.458893	-0.048351	2.954220
252.332330	2859.231515	17.463898	-0.048359	2.950393
252.424509	2851.265080	17.468903	-0.048371	2.946590
252.265303	2843.272247	17.473907	-0.048336	2.942756
252.439978	2835.276455	17.478912	-0.048363	2.938932
252.135180	2827.345720	17.483917	-0.048301	2.935111
252.144155	2819.326367	17.488922	-0.048297	2.931257
252.170704	2811.353245	17.493927	-0.048297	2.927422
252.026020	2803.387910	17.498931	-0.048265	2.923577
252.073481	2795.413381	17.503936	-0.048268	2.919732
252.048196	2787.459252	17.508941	-0.048258	2.915888
251.896768	2779.392106	17.513946	-0.048224	2.911978
251.871394	2771.381259	17.518951	-0.048214	2.908096
251.806603	2763.389329	17.523955	-0.048197	2.904217
251.862645	2755.470567	17.528960	-0.048202	2.900374
251.638960	2747.501489	17.533965	-0.048155	2.896486
251.585355	2739.509638	17.538970	-0.048140	2.892592
251.776175	2731.504631	17.543975	-0.048170	2.888699
251.508013	2723.540934	17.548979	-0.048115	2.884795
251.696368	2715.581309	17.553984	-0.048144	2.880914
251.632024	2707.611456	17.558989	-0.048127	2.877008
251.507819	2699.618429	17.563994	-0.048099	2.873083
251.573061	2691.631057	17.568999	-0.048105	2.869165
251.378606	2683.634204	17.574003	-0.048064	2.865223
251.473506	2675.676140	17.579008	-0.048076	2.861310
251.356492	2667.702144	17.584013	-0.048049	2.857373
251.251526	2659.721411	17.589018	-0.048024	2.853427
251.397858	2651.717068	17.594023	-0.048046	2.849478
251.346923	2643.748591	17.599027	-0.048031	2.845531
251.429864	2635.794272	17.604032	-0.048041	2.841592
251.372900	2627.841685	17.609037	-0.048025	2.837642
251.102015	2619.862408	17.614042	-0.047970	2.833660
250.979624	2611.860024	17.619047	-0.047942	2.829669
251.033916	2603.842569	17.624051	-0.047946	2.825676
251.203427	2595.870116	17.629056	-0.047973	2.821705
251.100078	2587.913832	17.634061	-0.047948	2.817722
250.818883	2579.953738	17.639066	-0.047890	2.813721
251.026298	2571.937768	17.644071	-0.047924	2.809714
250.717208	2563.983254	17.649075	-0.047861	2.805703
250.744423	2556.021984	17.654080	-0.047860	2.801701
250.891434	2548.033451	17.659085	-0.047882	2.797688
250.662563	2540.049051	17.664090	-0.047834	2.793649
250.716127	2532.059658	17.669095	-0.047839	2.789617
250.621961	2524.084742	17.674099	-0.047816	2.785579
250.861797	2516.094929	17.679104	-0.047855	2.781547
250.711429	2508.144172	17.684109	-0.047822	2.777506
250.589336	2500.176587	17.689114	-0.047794	2.773452
250.570455	2492.181670	17.694119	-0.047785	2.769384
250.505554	2484.206346	17.699123	-0.047768	2.765318
250.561482	2476.245134	17.704128	-0.047773	2.761260
250.473957	2468.296562	17.709133	-0.047751	2.757194
250.281889	2460.276331	17.714138	-0.047710	2.753079
250.223925	2452.249964	17.719143	-0.047694	2.748962
250.172352	2444.261644	17.724147	-0.047679	2.744860
250.234562	2436.324656	17.729152	-0.047685	2.740784
250.060656	2428.384964	17.734157	-0.047648	2.736687
249.986308	2420.376462	17.739162	-0.047628	2.732554
250.099538	2412.391072	17.744167	-0.047644	2.728438
250.029585	2404.421962	17.749171	-0.047626	2.724314
250.008195	2396.477847	17.754176	-0.047616	2.720198
250.058507	2388.511942	17.759181	-0.047620	2.716070
249.949599	2380.497273	17.764186	-0.047595	2.711900
249.947246	2372.533204	17.769191	-0.047589	2.707757
249.614613	2364.590998	17.774195	-0.047522	2.703598
249.680106	2356.591853	17.779200	-0.047529	2.699428
249.696817	2348.652683	17.784205	-0.047526	2.695280
249.516943	2340.658824	17.789210	-0.047488	2.691084
249.598156	2332.681722	17.794215	-0.047497	2.686908
249.558487	2324.690595	17.799219	-0.047485	2.682709
249.650666	2316.746455	17.804224	-0.047496	2.678537
249.560074	2308.775800	17.809229	-0.047474	2.674333
249.457702	2300.757661	17.814234	-0.047450	2.670096
249.424371	2292.797040	17.819239	-0.047438	2.665888
249.253832	2284.853348	17.824243	-0.047401	2.661673
249.488254	2276.853487	17.829248	-0.047440	2.657448
249.361448	2268.877465	17.834253	-0.047411	2.653205
249.186183	2260.899380	17.839258	-0.047373	2.648951
249.164676	2252.943760	17.844263	-0.047363	2.644712
248.985023	2245.014189	17.849267	-0.047325	2.640470
248.964302	2237.051055	17.854272	-0.047315	2.636214
248.972108	2229.043654	17.859277	-0.047311	2.631929
249.059000	2221.038362	17.864282	-0.047322	2.627643
249.126682	2213.087376	17.869287	-0.047330	2.623378
248.877395	2205.142402	17.874291	-0.047278	2.619089
248.836747	2197.183851	17.879296	-0.047265	2.614798
248.847127	2189.189845	17.884301	-0.047261	2.610486
248.648399	2181.223503	17.889306	-0.047219	2.606166
248.785342	2173.259785	17.894311	-0.047239	2.601864
248.723297	2165.291698	17.899315	-0.047222	2.597539
248.630225	2157.266138	17.904320	-0.047200	2.593173
248.435796	2149.179402	17.909325	-0.047158	2.588760
248.392382	2141.217558	17.914330	-0.047145	2.584417
248.494464	2133.311132	17.919335	-0.047158	2.580108
248.246628	2125.370864	17.924339	-0.047107	2.575748
248.424096	2117.400597	17.929344	-0.047135	2.571394
248.362166	2109.422177	17.934349	-0.047118	2.567012
248.204911	2101.493005	17.939354	-0.047083	2.562642
248.389081	2093.531428	17.944359	-0.047112	2.558271
248.442905	2085.542734	17.949363	-0.047117	2.553869
248.207644	2077.580178	17.954368	-0.047068	2.549453
248.035073	2069.633171	17.959373	-0.047030	2.545042
248.088933	2061.671788	17.964378	-0.047035	2.540632
248.179921	2053.708789	17.969383	-0.047047	2.536216
247.998761	2045.730702	17.974387	-0.047007	2.531764
247.859760	2037.780951	17.979392	-0.046976	2.527324
248.010274	2029.802043	17.984397	-0.046999	2.522879
247.832332	2021.862479	17.989402	-0.046960	2.518426
247.939617	2013.891530	17.994407	-0.046975	2.513967
247.623780	2005.896262	17.999411	-0.046911	2.509457
247.724021	1997.916885	18.004416	-0.046924	2.504977
247.787332	1989.964507	18.009421	-0.046931	2.500502
247.721034	1981.991661	18.014426	-0.046913	2.495997
247.714701	1974.034312	18.019431	-0.046907	2.491498
247.429582	1966.079818	18.024435	-0.046848	2.486972
247.414806	1958.132383	18.029440	-0.046840	2.482461
247.516119	1950.183487	18.034445	-0.046854	2.477950
247.301631	1942.213965	18.039450	-0.046808	2.473395
247.271127	1934.246478	18.044455	-0.046797	2.468847
247.182564	1926.264975	18.049459	-0.046775	2.464278
247.332385	1918.296846	18.054464	-0.046798	2.459727
247.023912	1910.398198	18.059469	-0.046735	2.455172
246.968025	1902.399612	18.064474	-0.046720	2.450570
247.060200	1894.434280	18.069479	-0.046731	2.445990
246.988167	1886.475662	18.074483	-0.046713	2.441392
247.008824	1878.509344	18.079488	-0.046711	2.436789
247.076876	1870.490145	18.084493	-0.046718	2.432150
246.959705	1862.508507	18.089498	-0.046691	2.427510
246.930446	1854.574295	18.094503	-0.046681	2.422895
246.876250	1846.624244	18.099507	-0.046665	2.418260
246.794809	1838.673835	18.104512	-0.046645	2.413613
246.701313	1830.709708	18.109517	-0.046622	2.408949
246.612036	1822.745058	18.114522	-0.046600	2.404276
246.671969	1814.814852	18.119527	-0.046606	2.399626
246.422493	1806.878940	18.124531	-0.046554	2.394939
246.423726	1798.900873	18.129536	-0.046549	2.390237
246.539438	1790.917631	18.134541	-0.046565	2.385533
246.650249	1782.942012	18.139546	-0.046580	2.380823
246.384623	1775.047074	18.144551	-0.046526	2.376122
246.190316	1767.082729	18.149555	-0.046484	2.371375
246.365935	1759.094361	18.154560	-0.046511	2.366635
246.105524	1751.191616	18.159565	-0.046458	2.361901
246.077081	1743.226337	18.164570	-0.046447	2.357139
246.074553	1735.260119	18.169575	-0.046441	2.352369
245.931603	1727.270838	18.174579	-0.046409	2.347563
245.874298	1719.325816	18.179584	-0.046393	2.342782
246.046590	1711.359669	18.184589	-0.046420	2.337997
245.916605	1703.401454	18.189594	-0.046391	2.333181
245.856492	1695.465183	18.194599	-0.046374	2.328375
245.876585	1687.503013	18.199603	-0.046372	2.323550
245.819416	1679.564052	18.204608	-0.046356	2.318723
245.719843	1671.629259	18.209613	-0.046333	2.313885
245.662287	1663.636093	18.214618	-0.046317	2.309004
245.712576	1655.691754	18.219623	-0.046321	2.304152
245.541142	1647.764246	18.224627	-0.046283	2.299281
245.472509	1639.814872	18.229632	-0.046265	2.294395
245.655082	1631.808095	18.234637	-0.046294	2.289484
245.526283	1623.885305	18.239642	-0.046265	2.284589
245.373627	1615.974537	18.244647	-0.046231	2.279688
245.456847	1608.015280	18.249651	-0.046241	2.274767
245.384584	1599.972574	18.254656	-0.046222	2.269770
245.294782	1592.038053	18.259661	-0.046200	2.264827
245.094530	1584.125473	18.264666	-0.046158	2.259878
245.216412	1576.168354	18.269671	-0.046175	2.254919
245.137411	1568.202054	18.274675	-0.046155	2.249925
244.984996	1560.274650	18.279680	-0.046121	2.244938
244.921999	1552.346523	18.284685	-0.046104	2.239947
244.852696	1544.408771	18.289690	-0.046086	2.234938
244.921378	1536.433989	18.294695	-0.046093	2.229907
244.788223	1528.475872	18.299699	-0.046063	2.224857
244.748091	1520.557006	18.304704	-0.046051	2.219829
244.828153	1512.616648	18.309709	-0.046060	2.214787
244.911661	1504.627770	18.314714	-0.046070	2.209702
244.743686	1496.714851	18.319719	-0.046034	2.204631
244.614721	1488.794525	18.324723	-0.046004	2.199548
244.420182	1480.866383	18.329728	-0.045963	2.194442
244.487631	1472.869823	18.334733	-0.045970	2.189304
244.562608	1464.885344	18.339738	-0.045979	2.184162
244.460502	1456.993206	18.344743	-0.045954	2.179051
244.261136	1449.059576	18.349747	-0.045912	2.173893
244.385050	1441.090754	18.354752	-0.045930	2.168729
244.333984	1433.159503	18.359757	-0.045915	2.163561
243.972270	1425.277434	18.364762	-0.045842	2.158384
244.084793	1417.306743	18.369767	-0.045858	2.153181
244.151939	1409.321763	18.374771	-0.045865	2.147951
244.075053	1401.402407	18.379776	-0.045845	2.142738
244.038906	1393.482794	18.384781	-0.045833	2.137517
243.894694	1385.532204	18.389786	-0.045801	2.132251
243.975597	1377.591339	18.394791	-0.045811	2.127001
243.877088	1369.659430	18.399795	-0.045787	2.121726
243.842359	1361.739041	18.404800	-0.045776	2.116452
243.862919	1353.747924	18.409805	-0.045774	2.111123
243.502545	1345.812201	18.414810	-0.045702	2.105781
243.614702	1337.879158	18.419815	-0.045717	2.100473
243.597103	1329.951938	18.424819	-0.045709	2.095142
243.575263	1322.001779	18.429824	-0.045699	2.089782
243.457347	1314.098204	18.434829	-0.045672	2.084430
243.364798	1306.177703	18.439834	-0.045649	2.079056
243.496672	1298.232407	18.444839	-0.045669	2.073673
243.379501	1290.288092	18.449843	-0.045641	2.068251
243.215508	1282.382932	18.454848	-0.045606	2.062838
243.236958	1274.459429	18.459853	-0.045604	2.057416
243.037646	1266.540500	18.464858	-0.045562	2.051961
243.215142	1258.569600	18.469863	-0.045590	2.046494
243.159610	1250.656999	18.474867	-0.045574	2.041029
242.893344	1242.772714	18.479872	-0.045519	2.035547
242.776337	1234.818890	18.484877	-0.045492	2.030017
242.644141	1226.878513	18.489882	-0.045462	2.024480
243.023745	1218.918803	18.494887	-0.045527	2.018966
242.714515	1211.034190	18.499891	-0.045465	2.013420
242.743281	1203.078826	18.504896	-0.045465	2.007843
242.842380	1195.156149	18.509901	-0.045478	2.002281
242.564995	1187.275220	18.514906	-0.045421	1.996693
242.711532	1179.317196	18.519911	-0.045443	1.991080
242.541105	1171.393899	18.524915	-0.045406	1.985442
242.505757	1163.492819	18.529920	-0.045394	1.979818
242.406763	1155.595057	18.534925	-0.045370	1.974174
242.404707	1147.635949	18.539930	-0.045364	1.968480
242.352345	1139.738217	18.544935	-0.045349	1.962808
242.177546	1131.851331	18.549939	-0.045312	1.957114
242.092689	1123.896483	18.554944	-0.045290	1.951365
241.979796	1115.957486	18.559949	-0.045264	1.945606
241.977953	1108.027511	18.564954	-0.045258	1.939849
242.037257	1100.119767	18.569959	-0.045264	1.934098
241.974326	1092.187715	18.574963	-0.045247	1.928299
241.947110	1084.283734	18.579968	-0.045237	1.922507
241.866176	1076.405528	18.584973	-0.045216	1.916710
241.804298	1068.449746	18.589978	-0.045200	1.910840
241.942295	1060.521685	18.594983	-0.045220	1.904995
241.784165	1052.647784	18.599987	-0.045185	1.899139
241.560918	1044.763102	18.604992	-0.045138	1.893250
241.604646	1036.829728	18.609997	-0.045141	1.887336
241.556576	1028.933246	18.615002	-0.045127	1.881420
241.347901	1021.069267	18.620007	-0.045083	1.875492
241.414718	1013.103417	18.625011	-0.045090	1.869500
241.271944	1005.206379	18.630016	-0.045058	1.863517
241.229596	997.321690	18.635021	-0.045045	1.857535
241.133344	989.403846	18.640026	-0.045022	1.851502
241.302254	981.468536	18.645031	-0.045048	1.845468
241.117315	973.612104	18.650035	-0.045008	1.839432
241.049264	965.720594	18.655040	-0.044990	1.833363
241.095098	957.784108	18.660045	-0.044993	1.827253
241.005300	949.893579	18.665050	-0.044971	1.821142
240.843140	942.026077	18.670055	-0.044936	1.815019
240.968810	934.086900	18.675059	-0.044954	1.808855
240.804444	926.228276	18.680064	-0.044918	1.802697
240.864345	918.344576	18.685069	-0.044924	1.796526
240.539984	910.419251	18.690074	-0.044858	1.790254
240.844963	902.470248	18.695079	-0.044910	1.784018
240.512323	894.642521	18.700083	-0.044843	1.777778
240.503822	886.728365	18.705088	-0.044836	1.771487
240.341258	878.863948	18.710093	-0.044800	1.765194
240.392528	870.968618	18.715098	-0.044804	1.758881
240.206290	863.109160	18.720103	-0.044765	1.752544
240.106468	855.208114	18.725107	-0.044741	1.746161
240.193623	847.314808	18.730112	-0.044752	1.739785
240.439295	839.409146	18.735117	-0.044792	1.733395
240.122383	831.548602	18.740122	-0.044728	1.726947
240.046555	823.693681	18.745127	-0.044708	1.720510
239.862553	815.846309	18.750131	-0.044669	1.714041
239.818419	807.925766	18.755136	-0.044655	1.707505
239.757876	800.067683	18.760141	-0.044639	1.700994
239.631682	792.201301	18.765146	-0.044610	1.694442
239.599152	784.318472	18.770151	-0.044599	1.687863
239.603850	776.435896	18.775155	-0.044594	1.681264
239.486574	768.589082	18.780160	-0.044567	1.674653
239.484207	760.711328	18.785165	-0.044561	1.668004
239.381367	752.841724	18.790170	-0.044537	1.661323
239.263187	744.998755	18.795175	-0.044510	1.654634
239.191974	737.127550	18.800179	-0.044491	1.647901
239.066123	729.275440	18.805184	-0.044463	1.641150
239.121544	721.421706	18.810189	-0.044468	1.634393
239.046081	713.485066	18.815194	-0.044448	1.627519
239.087107	705.634714	18.820199	-0.044451	1.620707
238.899565	697.811010	18.825203	-0.044411	1.613858
238.725685	689.961192	18.830208	-0.044373	1.606958
238.723064	682.118408	18.835213	-0.044367	1.600059
238.594349	674.283814	18.840218	-0.044338	1.593119
238.783763	666.396053	18.845223	-0.044368	1.586147
238.644610	658.571875	18.850227	-0.044337	1.579154
238.586991	650.731521	18.855232	-0.044321	1.572127
238.515140	642.892999	18.860237	-0.044302	1.565068
238.343006	635.090715	18.865242	-0.044265	1.557995
238.197053	627.255885	18.870247	-0.044232	1.550864
238.152743	619.408065	18.875251	-0.044219	1.543703
238.083123	611.575907	18.880256	-0.044201	1.536520
238.049460	603.739832	18.885261	-0.044189	1.529304
237.946999	595.911626	18.890266	-0.044165	1.522051
238.109713	588.077408	18.895271	-0.044190	1.514798
238.055391	580.245586	18.900275	-0.044175	1.507479
237.825373	572.454386	18.905280	-0.044127	1.500136
237.789759	564.651900	18.910285	-0.044115	1.492776
237.941742	556.784654	18.915290	-0.044138	1.485347
237.714409	549.026802	18.920295	-0.044090	1.477926
237.581666	541.190383	18.925299	-0.044060	1.470407
237.536844	533.361540	18.930304	-0.044047	1.462870
237.599817	525.558173	18.935309	-0.044053	1.455336
237.296454	517.778894	18.940314	-0.043991	1.447728
237.283136	509.990920	18.945319	-0.043984	1.440118
237.414165	502.174875	18.950323	-0.044003	1.432463
237.281697	494.387082	18.955328	-0.043973	1.424751
237.204211	486.624104	18.960333	-0.043953	1.417032
237.045704	478.842897	18.965338	-0.043919	1.409238
236.956606	471.077964	18.970343	-0.043897	1.401430
236.849956	463.312642	18.975347	-0.043872	1.393574
236.878075	455.493605	18.980352	-0.043872	1.385641
236.901954	447.729639	18.985357	-0.043871	1.377718
236.660351	439.973415	18.990362	-0.043821	1.369713
236.640950	432.209280	18.995367	-0.043812	1.361690
236.723372	424.437107	19.000371	-0.043822	1.353628
236.472611	416.699917	19.005376	-0.043770	1.345497
236.412616	408.969666	19.010381	-0.043754	1.337358
236.277118	401.220436	19.015386	-0.043724	1.329135
236.227025	393.479167	19.020391	-0.043709	1.320884
236.208272	385.694574	19.025395	-0.043700	1.312541
235.986113	377.895806	19.030400	-0.043654	1.304091
236.059638	370.157956	19.035405	-0.043662	1.295708
235.788424	362.463484	19.040410	-0.043607	1.287253
235.916098	354.730150	19.045415	-0.043625	1.278774
236.047423	346.994277	19.050419	-0.043644	1.270236
235.601716	339.351782	19.055424	-0.043556	1.261636
235.647693	331.640224	19.060429	-0.043560	1.252992
235.545511	323.945836	19.065434	-0.043535	1.244280
235.405350	316.278792	19.070439	-0.043504	1.235530
235.168278	308.593950	19.075443	-0.043455	1.226677
235.176126	300.900391	19.080448	-0.043451	1.217799
235.131302	293.221842	19.085453	-0.043438	1.208862
234.983662	285.561929	19.090458	-0.043405	1.199861
234.978998	277.899060	19.095463	-0.043399	1.190816
234.706094	270.272006	19.100467	-0.043343	1.181690
234.698225	262.611620	19.105472	-0.043337	1.172508
234.761684	254.950105	19.110477	-0.043343	1.163266
234.520802	247.339579	19.115482	-0.043293	1.153949
234.428485	239.689690	19.120487	-0.043271	1.144539
234.472923	232.047261	19.125491	-0.043274	1.135090
234.256820	224.445714	19.130496	-0.043229	1.125556
234.443318	216.818389	19.135501	-0.043258	1.115995
234.163319	209.253653	19.140506	-0.043201	1.106330
234.187288	201.662378	19.145511	-0.043201	1.096612
233.965570	194.104152	19.150515	-0.043154	1.086795
233.641129	186.583434	19.155520	-0.043089	1.076915
233.538685	179.020021	19.160525	-0.043065	1.066937
233.345674	171.478800	19.165530	-0.043024	1.056874
233.161287	163.951137	19.170535	-0.042984	1.046734
232.622689	156.508727	19.175539	-0.042879	1.036527
232.188651	149.031781	19.180544	-0.042793	1.026196
231.855330	141.566744	19.185549	-0.042726	1.015801
231.422045	134.102988	19.190554	-0.042640	1.005275
230.902450	126.680064	19.195559	-0.042539	0.994674
230.478565	119.210303	19.200563	-0.042455	0.983916
229.738717	111.833592	19.205568	-0.042312	0.973093
229.296813	104.422054	19.210573	-0.042225	0.962174
228.647063	97.056008	19.215578	-0.042099	0.951142
227.931331	89.709166	19.220583	-0.041961	0.939992
227.019143	82.401924	19.225587	-0.041786	0.928716
226.506514	75.047149	19.230592	-0.041686	0.917335
225.991458	67.701305	19.235597	-0.041585	0.905824
225.224802	60.648202	19.240602	-0.041437	0.894557