Fri Mar 12 13:00:53 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.390915	-0.020575	0.000000	-0.000029	0.719272

0.316194	-0.009259	0.005005	-0.000015	0.719268
0.501024	-0.036016	0.010010	-0.000049	0.719280
0.361994	-0.017797	0.015014	-0.000023	0.719267
0.489667	-0.036314	0.020019	-0.000047	0.719275
0.364855	-0.014019	0.025024	-0.000024	0.719275
0.346072	-0.012625	0.030029	-0.000020	0.719271
0.387194	-0.017469	0.035034	-0.000027	0.719275
0.131367	0.025509	0.040038	0.000020	0.719270
0.292286	-0.000472	0.045043	-0.000010	0.719275
0.165984	0.022761	0.050048	0.000014	0.719276
0.125888	0.026130	0.055053	0.000022	0.719269
0.318569	-0.003608	0.060058	-0.000014	0.719278
0.186802	0.015850	0.065062	0.000010	0.719270
0.173347	0.020805	0.070067	0.000013	0.719274
0.367776	-0.138582	0.075072	-0.000023	0.719028
0.235206	-0.151137	0.080077	0.000002	0.718956
0.380810	-0.171822	0.085082	-0.000025	0.718967
0.202502	-0.144072	0.090086	0.000008	0.718958
0.216917	-0.144160	0.095091	0.000006	0.718963
0.232751	-0.147072	0.100096	0.000003	0.718963
0.200343	-0.178017	0.105101	0.000009	0.718890
0.139272	-0.287839	0.110106	0.000021	0.718652
0.203687	-0.302725	0.115110	0.000009	0.718645
0.320130	-0.323041	0.120115	-0.000013	0.718645
0.301448	-0.320438	0.125120	-0.000009	0.718644
0.360907	-0.358478	0.130125	-0.000020	0.718589
0.486514	-0.497744	0.135130	-0.000043	0.718358
0.339394	-0.476573	0.140134	-0.000016	0.718348
0.480650	-0.498504	0.145139	-0.000042	0.718354
0.507712	-0.528391	0.150144	-0.000047	0.718305
0.371157	-0.649361	0.155149	-0.000021	0.718017
0.447884	-0.659366	0.160154	-0.000036	0.718024
0.163152	-0.613878	0.165158	0.000018	0.718014
0.014431	-0.659208	0.170163	0.000045	0.717872
0.342770	-0.800907	0.175168	-0.000016	0.717707
0.167011	-0.772931	0.180173	0.000017	0.717700
0.254883	-0.791556	0.185178	0.000001	0.717694
0.287073	-0.955954	0.190182	-0.000005	0.717380
0.348065	-0.967896	0.195187	-0.000016	0.717378
0.400811	-0.974383	0.200192	-0.000026	0.717383
0.299410	-1.108251	0.205197	-0.000007	0.717083
0.240393	-1.090847	0.210202	0.000004	0.717096
0.260994	-1.119974	0.215206	0.000001	0.717046
0.192846	-1.251057	0.220211	0.000014	0.716762
0.297281	-1.267700	0.225216	-0.000006	0.716766
0.019819	-1.285121	0.230221	0.000046	0.716633
-0.245612	-1.325682	0.235226	0.000096	0.716459
-0.287935	-1.321190	0.240230	0.000104	0.716453
-0.141086	-1.448644	0.245235	0.000076	0.716252
0.014693	-1.530386	0.250240	0.000048	0.716145
0.149434	-1.575360	0.255245	0.000023	0.716103
0.308473	-1.709743	0.260250	-0.000007	0.715893
0.139300	-1.683518	0.265254	0.000025	0.715885
0.204987	-1.831950	0.270259	0.000013	0.715613
0.283607	-1.875729	0.275264	-0.000002	0.715554
-0.114267	-1.901258	0.280269	0.000073	0.715363
-0.261713	-1.934543	0.285274	0.000100	0.715244
-0.114203	-2.015210	0.290278	0.000073	0.715136
-0.127633	-2.123721	0.295283	0.000076	0.714916
-0.270122	-2.117580	0.300288	0.000102	0.714878
-0.752803	-2.167338	0.305293	0.000192	0.714608
-0.694962	-2.173448	0.310298	0.000182	0.714616
-0.854195	-2.298187	0.315302	0.000211	0.714312
-0.598276	-2.360140	0.320307	0.000164	0.714279
-0.574065	-2.476479	0.325312	0.000160	0.714056
-3.670955	-1.969129	0.330317	0.000736	0.713968
-2.719201	-2.140868	0.335322	0.000559	0.713964
-3.081711	-2.230693	0.340326	0.000627	0.713656
-4.335514	-2.008026	0.345331	0.000860	0.713655
-3.832565	-2.095409	0.350336	0.000767	0.713659
-3.850920	-2.210573	0.355341	0.000770	0.713423
-4.868423	-2.057630	0.360346	0.000960	0.713367
-4.850596	-2.063957	0.365350	0.000956	0.713360
-4.489752	-2.170207	0.370355	0.000889	0.713277
-5.416278	-2.128396	0.375360	0.001062	0.713031
-5.563212	-2.105993	0.380365	0.001090	0.713023
-5.500954	-2.112901	0.385370	0.001078	0.713031
-5.402292	-2.193163	0.390374	0.001060	0.712906
-6.524775	-2.090767	0.395379	0.001269	0.712712
-6.090324	-2.164072	0.400384	0.001188	0.712720
-6.652949	-2.067991	0.405389	0.001293	0.712711
-6.462778	-2.116784	0.410394	0.001258	0.712682
-7.361041	-2.104542	0.415398	0.001425	0.712387
-7.330619	-2.110013	0.420403	0.001419	0.712387
-7.290538	-2.113326	0.425408	0.001412	0.712394
-7.779268	-2.031153	0.430413	0.001503	0.712384
-7.241099	-2.134854	0.435418	0.001403	0.712368
-7.828148	-2.168751	0.440422	0.001513	0.712092
-8.360959	-2.072608	0.445427	0.001612	0.712094
-8.502783	-2.046996	0.450432	0.001638	0.712095
-8.002514	-2.139164	0.455437	0.001545	0.712089
-7.890220	-2.154838	0.460442	0.001525	0.712097
-9.173807	-2.093181	0.465446	0.001764	0.711764
-9.293174	-2.073527	0.470451	0.001786	0.711760
-8.968479	-2.127677	0.475456	0.001726	0.711768
-9.291725	-2.075100	0.480461	0.001786	0.711757
-9.320978	-2.064222	0.485466	0.001792	0.711768
-9.165125	-2.097799	0.490470	0.001763	0.711757
-9.978430	-2.102362	0.495475	0.001914	0.711458
-10.001932	-2.094350	0.500480	0.001919	0.711466
-10.288359	-2.048565	0.505485	0.001972	0.711455
-9.880350	-2.117642	0.510490	0.001896	0.711462
-10.212289	-2.059913	0.515494	0.001958	0.711459
-10.186567	-2.064468	0.520499	0.001953	0.711459
-9.974028	-2.232442	0.525504	0.001914	0.711199
-11.384691	-2.012524	0.530509	0.002177	0.711136
-11.070847	-2.064394	0.535514	0.002118	0.711144
-10.538690	-2.160838	0.540518	0.002020	0.711141
-10.900581	-2.096440	0.545523	0.002087	0.711140
-10.783134	-2.115150	0.550528	0.002065	0.711144
-10.919806	-2.193504	0.555533	0.002091	0.710939
-11.487252	-2.122503	0.560538	0.002197	0.710879
-11.872719	-2.055817	0.565542	0.002268	0.710875
-11.964612	-2.038436	0.570547	0.002286	0.710876
-11.480033	-2.122259	0.575552	0.002196	0.710881
-11.606079	-2.104813	0.580557	0.002219	0.710871
-11.669697	-2.191570	0.585562	0.002231	0.710675
-12.819878	-2.055242	0.590566	0.002445	0.710538
-12.316272	-2.144920	0.595571	0.002352	0.710538
-12.310536	-2.143687	0.600576	0.002351	0.710542
-12.847952	-2.051249	0.605581	0.002451	0.710535
-12.366417	-2.133751	0.610586	0.002361	0.710541
-12.530234	-2.140793	0.615590	0.002392	0.710469
-13.477886	-2.097136	0.620595	0.002569	0.710219
-13.133212	-2.155681	0.625600	0.002505	0.710224
-13.830111	-2.034115	0.630605	0.002634	0.710219
-13.721658	-2.052594	0.635610	0.002614	0.710220
-13.089278	-2.166317	0.640614	0.002497	0.710218
-13.586645	-2.078200	0.645619	0.002589	0.710217
-13.781577	-2.105415	0.650624	0.002626	0.710093
-14.764910	-2.031940	0.655629	0.002809	0.709889
-14.204162	-2.130010	0.660634	0.002705	0.709892
-14.620168	-2.055454	0.665638	0.002782	0.709893
-14.882732	-2.010468	0.670643	0.002831	0.709889
-14.063510	-2.152806	0.675648	0.002679	0.709896
-14.414957	-2.092292	0.680653	0.002744	0.709892
-14.557234	-2.090450	0.685658	0.002771	0.709845
-15.208388	-2.097832	0.690662	0.002892	0.709598
-15.347834	-2.073772	0.695667	0.002918	0.709596
-15.286101	-2.081467	0.700672	0.002907	0.709602
-15.296185	-2.085027	0.705677	0.002909	0.709591
-14.842463	-2.160904	0.710682	0.002825	0.709601
-15.196136	-2.099524	0.715686	0.002891	0.709598
-15.460093	-2.112117	0.720691	0.002940	0.709478
-15.875819	-2.141066	0.725696	0.003017	0.709272
-15.917771	-2.139646	0.730701	0.003025	0.709259
-16.562661	-2.020472	0.735706	0.003145	0.709268
-16.209819	-2.085201	0.740710	0.003080	0.709264
-15.954810	-2.132415	0.745715	0.003033	0.709260
-16.128921	-2.097807	0.750720	0.003065	0.709267
-16.381908	-2.120514	0.755725	0.003112	0.709131
-16.865312	-2.119920	0.760730	0.003202	0.708960
-16.769390	-2.138781	0.765734	0.003185	0.708956
-17.420440	-2.023383	0.770739	0.003306	0.708954
-16.930344	-2.107778	0.775744	0.003215	0.708960
-16.886132	-2.119840	0.780749	0.003207	0.708951
-17.024215	-2.091654	0.785754	0.003233	0.708958
-17.029257	-2.175242	0.790758	0.003234	0.708789
-18.061385	-2.066166	0.795763	0.003426	0.708639
-18.032980	-2.067148	0.800768	0.003421	0.708647
-18.292676	-2.025510	0.805773	0.003469	0.708637
-18.105829	-2.055783	0.810778	0.003434	0.708643
-17.958361	-2.084415	0.815782	0.003407	0.708638
-18.272577	-2.029281	0.820787	0.003466	0.708636
-17.963050	-2.093967	0.825792	0.003408	0.708617
-18.710759	-2.095631	0.830797	0.003548	0.708346
-18.935818	-2.052023	0.835802	0.003590	0.708353
-18.925892	-2.054854	0.840806	0.003588	0.708351
-18.731982	-2.090478	0.845811	0.003552	0.708349
-18.745097	-2.083399	0.850816	0.003554	0.708358
-19.194967	-2.006967	0.855821	0.003638	0.708350
-18.825068	-2.071192	0.860826	0.003569	0.708353
-19.378971	-2.131757	0.865830	0.003673	0.708034
-20.272229	-1.984976	0.870835	0.003839	0.708009
-19.908010	-2.046049	0.875840	0.003771	0.708016
-19.687229	-2.090550	0.880845	0.003730	0.708006
-20.175159	-1.999195	0.885850	0.003821	0.708014
-20.151006	-2.004367	0.890854	0.003817	0.708012
-19.910432	-2.046945	0.895859	0.003772	0.708013
-19.728743	-2.126562	0.900864	0.003739	0.707918
-21.023116	-2.006477	0.905869	0.003980	0.707696
-20.627941	-2.073889	0.910874	0.003906	0.707702
-20.723966	-2.057757	0.915878	0.003924	0.707699
-21.148138	-1.984497	0.920883	0.004003	0.707695
-20.513766	-2.092715	0.925888	0.003885	0.707704
-20.812963	-2.043560	0.930893	0.003941	0.707695
-20.948435	-2.017322	0.935898	0.003966	0.707699
-21.128703	-2.135340	0.940902	0.004000	0.707398
-21.668781	-2.051337	0.945907	0.004101	0.707373
-21.700102	-2.040942	0.950912	0.004107	0.707383
-21.727334	-2.040649	0.955917	0.004112	0.707373
-21.581339	-2.063415	0.960922	0.004085	0.707380
-21.439532	-2.089636	0.965926	0.004059	0.707377
-21.802925	-2.028102	0.970931	0.004126	0.707371
-21.920692	-2.134364	0.975936	0.004148	0.707115
-22.273209	-2.090784	0.980941	0.004214	0.707076
-22.369313	-2.069816	0.985946	0.004232	0.707084
-22.400421	-2.066769	0.990950	0.004238	0.707079
-22.554135	-2.041208	0.995955	0.004267	0.707075
-22.016553	-2.133503	1.000960	0.004167	0.707082
-22.636641	-2.068392	1.005965	0.004282	0.706990
-23.624193	-2.009787	1.010970	0.004466	0.706754
-22.986478	-2.125531	1.015974	0.004348	0.706750
-23.758300	-1.991032	1.020979	0.004492	0.706743
-23.417652	-2.048422	1.025984	0.004428	0.706750
-23.051245	-2.117981	1.030989	0.004360	0.706741
-23.213176	-2.084736	1.035994	0.004390	0.706750
-23.127542	-2.139374	1.040998	0.004375	0.706670
-24.068865	-2.087009	1.046003	0.004550	0.706438
-23.699844	-2.147284	1.051008	0.004481	0.706449
-24.451838	-2.018141	1.056013	0.004621	0.706439
-24.213643	-2.059524	1.061018	0.004577	0.706441
-23.900129	-2.114527	1.066022	0.004519	0.706443
-24.544597	-2.000744	1.071027	0.004639	0.706440
-24.373779	-2.088219	1.076032	0.004607	0.706325
-25.140526	-2.053672	1.081037	0.004750	0.706120
-24.773133	-2.115874	1.086042	0.004682	0.706126
-25.123053	-2.052653	1.091046	0.004747	0.706128
-25.247643	-2.033987	1.096051	0.004771	0.706120
-24.446965	-2.171912	1.101056	0.004622	0.706130
-25.087367	-2.061724	1.106061	0.004741	0.706122
-25.417013	-2.075137	1.111066	0.004802	0.705976
-25.833814	-2.057086	1.116070	0.004880	0.705863
-25.795304	-2.066096	1.121075	0.004873	0.705858
-25.885568	-2.045358	1.126080	0.004890	0.705868
-25.740771	-2.076924	1.131085	0.004863	0.705856
-25.696870	-2.081501	1.136090	0.004855	0.705862
-25.983103	-2.029322	1.141094	0.004908	0.705864
-26.128672	-2.128130	1.146099	0.004936	0.705613
-26.494646	-2.104135	1.151104	0.005004	0.705530
-26.761783	-2.062458	1.156109	0.005054	0.705518
-26.612501	-2.084116	1.161114	0.005026	0.705527
-26.527351	-2.100973	1.166118	0.005010	0.705524
-26.756243	-2.062507	1.171123	0.005053	0.705519
-26.841958	-2.050301	1.176128	0.005069	0.705512
-27.420970	-2.099380	1.181133	0.005177	0.705206
-27.310041	-2.115986	1.186138	0.005157	0.705212
-27.702954	-2.044982	1.191142	0.005230	0.705214
-27.816414	-2.028604	1.196147	0.005251	0.705206
-27.155110	-2.142784	1.201152	0.005128	0.705213
-27.736734	-2.043216	1.206157	0.005236	0.705204
-27.743034	-2.065016	1.211162	0.005238	0.705158
-28.405018	-2.080775	1.216166	0.005361	0.704888
-28.433018	-2.078893	1.221171	0.005366	0.704882
-28.551731	-2.053167	1.226176	0.005389	0.704891
-28.297538	-2.102136	1.231181	0.005341	0.704883
-28.357234	-2.089062	1.236186	0.005353	0.704888
-28.574933	-2.048790	1.241190	0.005393	0.704891
-28.765319	-2.023074	1.246195	0.005429	0.704874
-28.806550	-2.154553	1.251200	0.005437	0.704594
-29.392623	-2.054572	1.256205	0.005546	0.704585
-29.829138	-1.973894	1.261210	0.005627	0.704590
-29.115551	-2.101393	1.266214	0.005495	0.704590
-29.446139	-2.046959	1.271219	0.005556	0.704580
-29.536975	-2.024539	1.276224	0.005573	0.704593
-29.561997	-2.022954	1.281229	0.005578	0.704587
-29.681252	-2.144839	1.286234	0.005600	0.704298
-30.143141	-2.078532	1.291238	0.005686	0.704265
-30.753365	-1.976060	1.296243	0.005800	0.704252
-30.157513	-2.077228	1.301248	0.005689	0.704262
-30.255587	-2.063315	1.306253	0.005708	0.704255
-30.311577	-2.050981	1.311258	0.005718	0.704260
-30.064398	-2.094556	1.316262	0.005672	0.704260
-30.712763	-2.124864	1.321267	0.005793	0.703966
-31.415152	-2.004601	1.326272	0.005924	0.703956
-31.315708	-2.025784	1.331277	0.005906	0.703949
-31.073234	-2.067670	1.336282	0.005861	0.703951
-31.260773	-2.031961	1.341286	0.005896	0.703955
-31.470370	-2.000832	1.346291	0.005935	0.703943
-30.856505	-2.104559	1.351296	0.005821	0.703954
-31.367017	-2.133381	1.356301	0.005916	0.703712
-32.266112	-2.013243	1.361306	0.006083	0.703631
-31.883990	-2.079796	1.366310	0.006012	0.703634
-31.793797	-2.098285	1.371315	0.005996	0.703629
-32.005816	-2.056471	1.376320	0.006035	0.703636
-32.145411	-2.035112	1.381325	0.006061	0.703629
-31.676738	-2.116091	1.386330	0.005974	0.703634
-32.124555	-2.177298	1.391334	0.006058	0.703349
-33.185635	-1.994309	1.396339	0.006255	0.703337
-33.022402	-2.018280	1.401344	0.006225	0.703347
-32.537803	-2.107707	1.406349	0.006135	0.703340
-32.947087	-2.033854	1.411354	0.006211	0.703342
-32.908203	-2.040217	1.416358	0.006204	0.703343
-32.876062	-2.067106	1.421363	0.006198	0.703300
-33.162284	-2.158521	1.426368	0.006252	0.703012
-33.500022	-2.102718	1.431373	0.006315	0.703003
-33.808252	-2.048582	1.436378	0.006372	0.703001
-33.583066	-2.084684	1.441382	0.006330	0.703009
-33.949789	-2.022477	1.446387	0.006399	0.703002
-33.641470	-2.073324	1.451392	0.006341	0.703011
-33.634275	-2.134279	1.456397	0.006340	0.702890
-35.027476	-1.983077	1.461402	0.006600	0.702693
-34.420344	-2.091340	1.466406	0.006487	0.702693
-34.616783	-2.059415	1.471411	0.006523	0.702686
-34.540417	-2.068444	1.476416	0.006509	0.702696
-34.602959	-2.060856	1.481421	0.006521	0.702688
-34.595845	-2.060473	1.486426	0.006520	0.702691
-34.318673	-2.170001	1.491430	0.006468	0.702570
-35.781944	-2.010539	1.496435	0.006741	0.702364
-35.355510	-2.080871	1.501440	0.006662	0.702376
-35.476444	-2.062522	1.506445	0.006684	0.702369
-35.730017	-2.017009	1.511450	0.006732	0.702369
-35.282781	-2.093173	1.516454	0.006648	0.702376
-35.336162	-2.087371	1.521459	0.006659	0.702369
-35.395234	-2.140236	1.526464	0.006670	0.702240
-36.503974	-2.026106	1.531469	0.006876	0.702071
-36.178595	-2.082321	1.536474	0.006816	0.702074
-36.090837	-2.095547	1.541478	0.006799	0.702079
-36.715537	-1.988758	1.546483	0.006916	0.702070
-36.126460	-2.088172	1.551488	0.006806	0.702081
-36.259511	-2.067043	1.556493	0.006831	0.702075
-36.635343	-2.076400	1.561498	0.006901	0.701921
-37.372382	-2.030357	1.566502	0.007039	0.701748
-37.133198	-2.077259	1.571507	0.006994	0.701739
-36.905848	-2.113874	1.576512	0.006952	0.701746
-37.391566	-2.029587	1.581517	0.007043	0.701742
-37.058825	-2.087464	1.586522	0.006981	0.701744
-36.928083	-2.108125	1.591526	0.006956	0.701749
-37.409350	-2.122976	1.596531	0.007046	0.701546
-38.278291	-2.019049	1.601536	0.007208	0.701442
-38.018587	-2.069494	1.606541	0.007160	0.701433
-37.911352	-2.089088	1.611546	0.007140	0.701432
-38.069468	-2.055775	1.616550	0.007170	0.701442
-38.057157	-2.062722	1.621555	0.007167	0.701433
-37.982794	-2.071943	1.626560	0.007154	0.701441
-38.347182	-2.100534	1.631565	0.007222	0.701251
-39.283332	-1.998162	1.636570	0.007396	0.701120
-38.647644	-2.107405	1.641574	0.007278	0.701128
-39.060405	-2.037471	1.646579	0.007355	0.701120
-39.064806	-2.032033	1.651584	0.007356	0.701130
-38.725507	-2.096092	1.656589	0.007293	0.701122
-38.817053	-2.079622	1.661594	0.007310	0.701122
-38.941730	-2.139664	1.666598	0.007333	0.700955
-39.631693	-2.060322	1.671603	0.007462	0.700867
-39.404792	-2.095246	1.676608	0.007420	0.700878
-39.587002	-2.067001	1.681613	0.007454	0.700869
-39.536797	-2.075385	1.686618	0.007444	0.700870
-39.270157	-2.118397	1.691622	0.007395	0.700879
-39.762012	-2.114626	1.696627	0.007486	0.700708
-41.061810	-1.966790	1.701632	0.007729	0.700538
-40.284444	-2.106042	1.706637	0.007584	0.700537
-40.267265	-2.109962	1.711642	0.007581	0.700535
-40.638071	-2.040265	1.716646	0.007650	0.700542
-40.692761	-2.036490	1.721651	0.007660	0.700529
-40.461323	-2.072573	1.726656	0.007617	0.700540
-40.651386	-2.130543	1.731661	0.007653	0.700353
-41.706639	-2.008066	1.736666	0.007849	0.700220
-41.247245	-2.086768	1.741670	0.007764	0.700226
-41.494293	-2.046183	1.746675	0.007810	0.700219
-41.492231	-2.044251	1.751680	0.007810	0.700223
-41.070308	-2.120812	1.756685	0.007731	0.700220
-41.424461	-2.059819	1.761690	0.007797	0.700216
-41.625403	-2.142119	1.766694	0.007835	0.699976
-42.289613	-2.066259	1.771699	0.007959	0.699889
-41.998771	-2.115443	1.776704	0.007905	0.699894
-42.083237	-2.099773	1.781709	0.007921	0.699895
-42.573106	-2.012228	1.786714	0.008012	0.699896
-42.232493	-2.069135	1.791718	0.007949	0.699903
-42.118843	-2.099529	1.796723	0.007928	0.699882
-42.922839	-2.091753	1.801728	0.008077	0.699607
-43.002267	-2.080173	1.806733	0.008092	0.699602
-43.217853	-2.043003	1.811738	0.008132	0.699599
-43.039462	-2.071097	1.816742	0.008099	0.699606
-43.370817	-2.017395	1.821747	0.008161	0.699595
-43.120597	-2.058645	1.826752	0.008115	0.699602
-42.961996	-2.108355	1.831757	0.008085	0.699558
-44.149227	-2.040809	1.836762	0.008306	0.699265
-43.764510	-2.104819	1.841766	0.008235	0.699274
-44.197730	-2.032561	1.846771	0.008316	0.699264
-44.020031	-2.059612	1.851776	0.008283	0.699273
-43.854600	-2.090163	1.856781	0.008252	0.699270
-44.016749	-2.063828	1.861786	0.008282	0.699265
-43.978458	-2.088651	1.866790	0.008275	0.699228
-44.805247	-2.075211	1.871795	0.008429	0.698956
-44.588086	-2.109840	1.876800	0.008389	0.698964
-44.862211	-2.063380	1.881805	0.008440	0.698959
-45.087682	-2.023906	1.886810	0.008482	0.698957
-44.680452	-2.092242	1.891814	0.008407	0.698965
-44.887570	-2.058615	1.896819	0.008445	0.698959
-44.824308	-2.114653	1.901824	0.008434	0.698867
-45.713345	-2.065158	1.906829	0.008599	0.698645
-45.555835	-2.095064	1.911834	0.008570	0.698642
-45.632680	-2.076837	1.916838	0.008584	0.698651
-45.974659	-2.021228	1.921843	0.008648	0.698639
-45.825969	-2.044109	1.926848	0.008621	0.698647
-45.597825	-2.086152	1.931853	0.008578	0.698644
-45.727845	-2.118599	1.936858	0.008603	0.698530
-46.087988	-2.137281	1.941862	0.008670	0.698361
-46.172858	-2.127871	1.946867	0.008686	0.698350
-46.429003	-2.080045	1.951872	0.008734	0.698354
-46.326617	-2.097970	1.956877	0.008715	0.698354
-46.357303	-2.093964	1.961882	0.008720	0.698351
-46.427046	-2.095081	1.966886	0.008733	0.698323
-47.373973	-2.078051	1.971891	0.008910	0.698014
-46.932994	-2.153530	1.976896	0.008828	0.698020
-47.398963	-2.071579	1.981901	0.008915	0.698018
-47.784870	-2.004598	1.986906	0.008987	0.698014
-47.299746	-2.086224	1.991910	0.008897	0.698024
-47.140374	-2.120182	1.996915	0.008867	0.698012
-47.828312	-2.093110	2.001920	0.008995	0.697817

-47.972672	-2.124277	2.011917	0.009022	0.697701
-48.343494	-2.057501	2.021914	0.009092	0.697702
-48.356249	-2.055052	2.031910	0.009094	0.697702
-48.274032	-2.069159	2.041907	0.009079	0.697702
-48.483728	-2.031545	2.051904	0.009118	0.697702
-48.337664	-2.056541	2.061901	0.009091	0.697704
-48.362068	-2.053319	2.071898	0.009096	0.697701
-48.192960	-2.082003	2.081894	0.009065	0.697704
-48.233908	-2.073681	2.091891	0.009073	0.697706
-48.331864	-2.056304	2.101888	0.009091	0.697705
-47.728521	-2.082657	2.111885	0.008979	0.697870
-47.553505	-2.041618	2.121882	0.008947	0.698017
-47.280621	-2.091576	2.131878	0.008896	0.698014
-47.322938	-2.081819	2.141875	0.008904	0.698018
-47.437057	-2.061368	2.151872	0.008926	0.698017
-47.247360	-2.094836	2.161869	0.008891	0.698018
-47.395401	-2.005419	2.171866	0.008918	0.698145
-46.358989	-2.086324	2.181862	0.008726	0.698356
-46.362392	-2.085928	2.191859	0.008726	0.698356
-46.252916	-2.104973	2.201856	0.008706	0.698356
-46.530232	-2.053801	2.211853	0.008758	0.698359
-46.002020	-2.034421	2.221850	0.008660	0.698590
-45.726817	-2.057498	2.231846	0.008609	0.698642
-45.710215	-2.059709	2.241843	0.008606	0.698643
-45.748789	-2.045812	2.251840	0.008613	0.698657
-44.765838	-2.072254	2.261837	0.008431	0.698959
-44.862324	-2.055065	2.271834	0.008449	0.698959
-44.726380	-2.079636	2.281830	0.008424	0.698958
-44.876121	-2.008832	2.291827	0.008452	0.699047
-43.756535	-2.098801	2.301824	0.008244	0.699269
-44.039602	-2.047836	2.311821	0.008297	0.699270
-44.041833	-2.048496	2.321818	0.008297	0.699267
-43.360156	-2.052399	2.331814	0.008171	0.699506
-43.302547	-2.017114	2.341811	0.008160	0.699598
-43.224782	-2.029539	2.351808	0.008146	0.699600
-42.860274	-2.063303	2.361805	0.008078	0.699663
-42.280738	-2.051806	2.371802	0.007970	0.699896
-42.038878	-2.094957	2.381798	0.007926	0.699895
-42.305552	-2.045261	2.391795	0.007975	0.699899
-41.575845	-2.089861	2.401792	0.007840	0.700072
-41.230980	-2.078329	2.411789	0.007776	0.700220
-41.502471	-2.029470	2.421786	0.007827	0.700221
-41.331766	-2.057080	2.431782	0.007795	0.700226
-40.614908	-2.032039	2.441779	0.007662	0.700535
-40.292719	-2.088203	2.451776	0.007602	0.700538
-40.431053	-2.063052	2.461773	0.007628	0.700538
-40.113214	-2.047266	2.471770	0.007569	0.700685
-39.430991	-2.075846	2.481766	0.007442	0.700873
-39.615631	-2.041242	2.491763	0.007477	0.700876
-39.293050	-2.097011	2.501760	0.007417	0.700879
-39.143164	-2.024268	2.511757	0.007389	0.701080
-38.665468	-2.087440	2.521754	0.007301	0.701124
-38.709652	-2.080159	2.531750	0.007309	0.701123
-38.641350	-2.025174	2.541747	0.007296	0.701258
-37.666995	-2.108350	2.551744	0.007115	0.701441
-37.897833	-2.067013	2.561741	0.007159	0.701441
-37.732151	-2.097658	2.571738	0.007128	0.701438
-37.114119	-2.061156	2.581734	0.007013	0.701735
-37.096546	-2.057744	2.591731	0.007010	0.701748
-36.768876	-2.115419	2.601728	0.006949	0.701749
-36.850936	-2.015326	2.611725	0.006965	0.701921
-35.959099	-2.096751	2.621722	0.006799	0.702078
-36.243675	-2.045564	2.631718	0.006852	0.702078
-36.117190	-2.050865	2.641715	0.006829	0.702113
-35.235421	-2.075850	2.651712	0.006665	0.702380
-35.272002	-2.071087	2.661709	0.006672	0.702376
-35.393849	-2.049767	2.671706	0.006695	0.702374
-34.879100	-2.022213	2.681702	0.006599	0.702615
-34.337042	-2.077193	2.691699	0.006498	0.702699
-34.238249	-2.094403	2.701696	0.006480	0.702699
-34.394222	-2.036289	2.711693	0.006509	0.702760
-33.538090	-2.065933	2.721690	0.006350	0.703008
-33.714821	-2.035294	2.731686	0.006383	0.703006
-33.488840	-2.073826	2.741683	0.006342	0.703009
-32.990639	-2.020172	2.751680	0.006249	0.703296
-32.803875	-2.028793	2.761677	0.006214	0.703346
-32.589227	-2.069097	2.771674	0.006175	0.703341
-32.448237	-2.032812	2.781670	0.006149	0.703465
-31.745146	-2.072682	2.791667	0.006018	0.703637
-31.936895	-2.036269	2.801664	0.006054	0.703641
-31.885463	-2.045110	2.811661	0.006045	0.703641
-31.219021	-2.008295	2.821658	0.005921	0.703955
-31.034209	-2.041614	2.831654	0.005886	0.703954
-30.840408	-2.076652	2.841651	0.005851	0.703952
-30.541706	-2.035444	2.851648	0.005795	0.704142
-30.199141	-2.036418	2.861645	0.005732	0.704263
-30.139767	-2.048342	2.871642	0.005721	0.704260
-29.981887	-2.054180	2.881638	0.005692	0.704304
-29.076443	-2.073545	2.891635	0.005523	0.704590
-29.274965	-2.037320	2.901632	0.005560	0.704592
-29.053087	-2.076664	2.911629	0.005519	0.704592
-28.812112	-2.037333	2.921626	0.005475	0.704757
-28.451887	-2.035422	2.931622	0.005408	0.704890
-28.463315	-2.033366	2.941619	0.005410	0.704889
-28.472109	-1.997050	2.951616	0.005412	0.704959
-27.596577	-2.026468	2.961613	0.005249	0.705213
-27.423968	-2.057648	2.971610	0.005217	0.705212
-27.669869	-2.012900	2.981606	0.005263	0.705214
-26.738078	-2.044490	2.991603	0.005090	0.705484
-26.749970	-2.020603	3.001600	0.005093	0.705527
-26.373887	-2.088250	3.011597	0.005023	0.705526
-26.624385	-2.002327	3.021594	0.005070	0.705608
-25.656372	-2.047596	3.031590	0.004890	0.705864
-25.406509	-2.092275	3.041587	0.004843	0.705863
-25.726018	-2.033979	3.051584	0.004903	0.705865
-25.340668	-2.018243	3.061581	0.004831	0.706035
-24.995916	-2.034202	3.071578	0.004767	0.706126
-25.064819	-2.020969	3.081574	0.004781	0.706127
-24.660613	-2.044332	3.091571	0.004705	0.706225
-24.103017	-2.033547	3.101568	0.004602	0.706446
-24.021071	-2.047981	3.111565	0.004587	0.706446
-24.317335	-1.996397	3.121562	0.004642	0.706443
-23.368166	-2.011954	3.131558	0.004466	0.706751
-23.173731	-2.045234	3.141555	0.004430	0.706753
-23.227314	-2.034848	3.151552	0.004440	0.706755
-22.683159	-2.031424	3.161549	0.004339	0.706956
-22.521544	-1.997195	3.171546	0.004309	0.707082
-22.382638	-2.021392	3.181542	0.004283	0.707083
-22.225213	-2.027401	3.191539	0.004254	0.707127
-21.544310	-2.021696	3.201536	0.004128	0.707381
-21.422135	-2.043261	3.211533	0.004105	0.707381
-21.611327	-2.011468	3.221530	0.004141	0.707377
-20.783319	-2.044907	3.231526	0.003987	0.707605
-20.719934	-2.009239	3.241523	0.003975	0.707699
-20.628176	-2.024174	3.251520	0.003958	0.707702
-20.586134	-1.986449	3.261517	0.003951	0.707792
-19.616893	-2.049315	3.271514	0.003770	0.708012
-19.743381	-2.024882	3.281510	0.003794	0.708015
-19.691749	-2.031962	3.291507	0.003785	0.708019
-19.119458	-2.013469	3.301504	0.003678	0.708260
-18.604012	-2.057431	3.311501	0.003583	0.708356
-18.950470	-1.996521	3.321498	0.003647	0.708354
-18.614895	-2.046486	3.331494	0.003585	0.708373
-18.292184	-1.970842	3.341491	0.003525	0.708639
-17.752002	-2.066360	3.351488	0.003425	0.708640
-17.802060	-2.055822	3.361485	0.003434	0.708643
-17.521986	-2.012884	3.371482	0.003382	0.708829
-16.937439	-2.053151	3.381478	0.003274	0.708956
-16.982730	-2.045335	3.391475	0.003282	0.708955
-17.104922	-2.013547	3.401472	0.003305	0.708975
-16.400850	-1.992667	3.411469	0.003175	0.709267
-16.244516	-2.020591	3.421466	0.003146	0.709267
-16.125946	-2.043775	3.431462	0.003124	0.709262
-15.783235	-1.994529	3.441459	0.003060	0.709483
-15.352781	-2.014262	3.451456	0.002980	0.709596
-15.333042	-2.017138	3.461453	0.002977	0.709597
-15.314461	-1.990658	3.471450	0.002974	0.709656
-14.534403	-2.010727	3.481446	0.002829	0.709894
-14.613930	-1.995599	3.491443	0.002844	0.709895
-14.366511	-2.038660	3.501440	0.002798	0.709897
-13.982041	-1.971175	3.511437	0.002726	0.710168
-13.665292	-2.001247	3.521434	0.002668	0.710220
-13.344796	-2.059050	3.531430	0.002608	0.710219
-13.509230	-1.981426	3.541427	0.002639	0.710315
-12.305091	-2.084929	3.551424	0.002415	0.710536
-12.601044	-2.029434	3.561421	0.002470	0.710541
-12.863112	-1.984985	3.571418	0.002519	0.710536
-12.036764	-2.026918	3.581414	0.002366	0.710746
-11.955728	-1.975385	3.591411	0.002351	0.710878
-11.804470	-2.002166	3.601408	0.002323	0.710878
-11.840319	-1.965069	3.611405	0.002330	0.710938
-10.974071	-2.017061	3.621402	0.002169	0.711142
-11.055885	-2.002740	3.631398	0.002184	0.711141
-11.138229	-1.987110	3.641395	0.002200	0.711143
-10.325585	-1.990144	3.651392	0.002049	0.711425
-10.131698	-2.007125	3.661389	0.002013	0.711460
-10.247845	-1.986021	3.671386	0.002035	0.711460
-9.845192	-1.989455	3.681382	0.001960	0.711596
-9.144053	-2.030462	3.691379	0.001830	0.711763
-9.229558	-2.014779	3.701376	0.001846	0.711764
-9.445440	-1.975824	3.711373	0.001886	0.711764
-8.427770	-1.993177	3.721370	0.001697	0.712091
-8.540162	-1.971448	3.731366	0.001718	0.712093
-8.157785	-2.039723	3.741363	0.001647	0.712093
-8.053634	-1.985195	3.751360	0.001628	0.712238
-7.118867	-2.073944	3.761357	0.001454	0.712393
-7.002482	-2.095569	3.771354	0.001433	0.712390
-7.268638	-2.048246	3.781350	0.001482	0.712390
-7.028861	-2.016478	3.791347	0.001438	0.712538
-5.946853	-2.120748	3.801344	0.001237	0.712714
-6.308997	-2.056873	3.811341	0.001304	0.712712
-6.268476	-2.062782	3.821338	0.001297	0.712714
-5.875250	-2.031855	3.831334	0.001224	0.712915
-5.183023	-2.095802	3.841331	0.001095	0.713032
-5.232595	-2.086561	3.851328	0.001105	0.713033
-5.084815	-2.112955	3.861325	0.001078	0.713032
-4.488052	-2.103432	3.871322	0.000967	0.713262
-4.268316	-2.091099	3.881318	0.000926	0.713364
-4.207085	-2.101364	3.891315	0.000915	0.713365
-4.046934	-2.128625	3.901312	0.000885	0.713367
-3.905305	-2.066212	3.911309	0.000859	0.713541
-3.402162	-2.099319	3.921306	0.000766	0.713653
-3.595332	-2.062450	3.931302	0.000802	0.713658
-3.197697	-2.132337	3.941299	0.000728	0.713659
-2.704241	-2.067804	3.951296	0.000636	0.713962
-2.585396	-2.082434	3.961293	0.000614	0.713974
-2.553885	-2.087325	3.971290	0.000609	0.713975
-2.447555	-2.050799	3.981286	0.000589	0.714085
-1.857075	-2.057951	3.991283	0.000479	0.714279
-1.931843	-2.043042	4.001280	0.000494	0.714282
-1.676393	-2.073822	4.011277	0.000446	0.714311
-1.690893	-1.921362	4.021274	0.000449	0.714608
-1.515357	-1.950769	4.031270	0.000417	0.714611
-1.686987	-1.866207	4.041267	0.000449	0.714718
-1.279587	-1.840572	4.051264	0.000373	0.714913
-1.192410	-1.856048	4.061261	0.000357	0.714912
-1.165039	-1.714899	4.071258	0.000352	0.715202
-1.258616	-1.681312	4.081254	0.000370	0.715235
-1.091030	-1.587620	4.091251	0.000339	0.715479
-1.007352	-1.566212	4.101248	0.000323	0.715551
-1.085976	-1.411254	4.111245	0.000338	0.715830
-1.297933	-1.325926	4.121242	0.000378	0.715924
-0.662447	-1.332110	4.131238	0.000260	0.716136
-0.941792	-1.208520	4.141235	0.000312	0.716281
-0.850131	-1.139126	4.151232	0.000295	0.716451
-0.678645	-1.019937	4.161229	0.000263	0.716747
-0.839413	-0.901652	4.171226	0.000293	0.716924
-0.279435	-0.904973	4.181222	0.000189	0.717114
-0.470093	-0.733782	4.191219	0.000225	0.717385
-0.645383	-0.579904	4.201216	0.000257	0.717627
-0.476290	-0.487999	4.211213	0.000226	0.717868
-0.684506	-0.320857	4.221210	0.000265	0.718125
-0.290934	-0.250763	4.231206	0.000192	0.718401
-0.352251	-0.109611	4.241203	0.000203	0.718658
-0.085789	-0.000771	4.251200	0.000154	0.718966
-0.148896	0.152768	4.261197	0.000166	0.719246
0.000000	0.281057	4.271194	0.000138	0.719551

0.084638	0.888751	4.276198	0.000122	0.720778
0.287908	2.102960	4.281203	0.000084	0.723235
0.535078	3.906288	4.286208	0.000037	0.726849
0.885127	6.252751	4.291213	-0.000030	0.731535
0.931492	9.152233	4.296218	-0.000040	0.737153
1.378398	12.460044	4.301222	-0.000126	0.743643
2.030026	16.191096	4.306227	-0.000249	0.750945
2.043386	20.442003	4.311232	-0.000254	0.758938
2.636993	24.987810	4.316237	-0.000368	0.767582
3.058290	29.929258	4.321242	-0.000449	0.776798
3.566875	35.201629	4.326246	-0.000547	0.786530
4.180395	40.783417	4.331251	-0.000665	0.796727
4.820648	46.651905	4.336256	-0.000788	0.807307
5.505159	52.819570	4.341261	-0.000919	0.818282
5.966442	59.284899	4.346266	-0.001009	0.829553
6.386903	65.994106	4.351270	-0.001092	0.841072
6.826173	72.913331	4.356275	-0.001178	0.852791
7.052704	80.067991	4.361280	-0.001225	0.864675
9.432209	87.050926	4.366285	-0.001672	0.876732
12.104547	94.184467	4.371290	-0.002175	0.888948
12.713288	101.872422	4.376294	-0.002293	0.901298
13.539340	109.666755	4.381299	-0.002452	0.913705
13.993760	117.629878	4.386304	-0.002541	0.926105
14.663442	125.674615	4.391309	-0.002671	0.938520
15.998790	133.705358	4.396314	-0.002925	0.950926
17.534800	141.806583	4.401318	-0.003216	0.963327
18.195503	150.153964	4.406323	-0.003344	0.975705
18.811277	158.576114	4.411328	-0.003464	0.988023
19.990518	166.970335	4.416333	-0.003689	1.000289
20.711766	175.455062	4.421338	-0.003829	1.012421
21.772816	183.950404	4.426342	-0.004032	1.024505
22.557814	192.532000	4.431347	-0.004184	1.036500
23.191634	201.145327	4.436352	-0.004307	1.048365
24.373479	209.716927	4.441357	-0.004533	1.060167
25.001241	218.392010	4.446362	-0.004655	1.071850
25.612572	227.052484	4.451366	-0.004775	1.083383
26.526380	235.680851	4.456371	-0.004950	1.094820
27.205620	244.337507	4.461376	-0.005082	1.106123
28.180305	252.969326	4.466381	-0.005269	1.117344
28.709819	261.658585	4.471386	-0.005373	1.128429
29.732498	270.274479	4.476390	-0.005569	1.139420
30.599033	278.934182	4.481395	-0.005736	1.150327
31.072534	287.628406	4.486400	-0.005830	1.161090
31.822814	296.257157	4.491405	-0.005975	1.171733
32.458383	304.873481	4.496410	-0.006099	1.182241
33.106039	313.502744	4.501414	-0.006225	1.192674
33.821240	322.088217	4.506419	-0.006364	1.202978
34.287855	330.713135	4.511424	-0.006456	1.213191
34.779918	339.323996	4.516429	-0.006553	1.223307
35.743107	347.852065	4.521434	-0.006738	1.233336
36.995410	356.305608	4.526438	-0.006977	1.243255
37.220919	364.929435	4.531443	-0.007024	1.253091
37.991197	373.425623	4.536448	-0.007173	1.262811
38.890989	381.913473	4.541453	-0.007346	1.272470
39.385832	390.430877	4.546458	-0.007444	1.282014
39.793263	398.963538	4.551462	-0.007525	1.291488
40.484726	407.425411	4.556467	-0.007659	1.300867
41.098041	415.941779	4.561472	-0.007779	1.310224
41.790326	424.456148	4.566477	-0.007913	1.319526
42.504338	432.840530	4.571482	-0.008051	1.328628
43.093038	441.274211	4.576486	-0.008166	1.337697
43.502020	449.707139	4.581491	-0.008248	1.346673
43.835935	458.143624	4.586496	-0.008315	1.355580
44.468509	466.511311	4.591501	-0.008438	1.364409
44.796580	474.932476	4.596506	-0.008505	1.373184
45.355307	483.284218	4.601510	-0.008614	1.381871
45.975229	491.649728	4.606515	-0.008735	1.390528
46.606701	499.988020	4.611520	-0.008858	1.399105
47.137816	508.334029	4.616525	-0.008962	1.407621
47.556874	516.696943	4.621530	-0.009046	1.416084
47.997007	525.033343	4.626534	-0.009133	1.424473
48.449368	533.392015	4.631539	-0.009222	1.432837
48.993776	541.687439	4.636544	-0.009329	1.441106
49.687925	549.983376	4.641549	-0.009464	1.449351
50.244943	558.293133	4.646554	-0.009573	1.457541
50.649050	566.599362	4.651558	-0.009653	1.465657
51.132190	574.958455	4.656563	-0.009749	1.473792
51.478035	583.243281	4.661568	-0.009818	1.481789
51.681649	591.563681	4.666573	-0.009861	1.489755
52.269538	599.807251	4.671578	-0.009976	1.497665
52.976517	608.027522	4.676582	-0.010113	1.505530
53.637804	616.285859	4.681587	-0.010241	1.513382
54.008339	624.546839	4.686592	-0.010316	1.521152
54.609196	632.790563	4.691597	-0.010433	1.528901
55.011930	641.059664	4.696602	-0.010513	1.536605
55.669468	649.284909	4.701606	-0.010641	1.544267
56.070548	657.572052	4.706611	-0.010721	1.551910
56.545987	665.802304	4.711616	-0.010815	1.559475
56.870444	674.055595	4.716621	-0.010880	1.567001
57.160411	682.319884	4.721626	-0.010939	1.574497
57.909380	690.492259	4.726630	-0.011084	1.581941
58.524599	698.700552	4.731635	-0.011204	1.589362
59.024387	706.914992	4.736640	-0.011302	1.596738
59.504975	715.134717	4.741645	-0.011397	1.604081
59.980452	723.357844	4.746650	-0.011491	1.611394
60.632970	731.555412	4.751654	-0.011617	1.618675
60.966329	739.794093	4.756659	-0.011685	1.625915
61.295601	748.082455	4.761664	-0.011751	1.633165
61.827610	756.262002	4.766669	-0.011856	1.640317
62.150639	764.460001	4.771674	-0.011921	1.647425
62.670302	772.653567	4.776678	-0.012023	1.654526
63.248415	780.817798	4.781683	-0.012136	1.661578
63.618218	789.005418	4.786688	-0.012210	1.668593
64.377376	797.171899	4.791693	-0.012357	1.675612
64.776728	805.342398	4.796698	-0.012436	1.682557
65.215101	813.528660	4.801702	-0.012523	1.689492
65.649077	821.727510	4.806707	-0.012609	1.696409
66.054917	829.901681	4.811712	-0.012690	1.703273
66.261997	838.139300	4.816717	-0.012734	1.710135
66.510770	846.337280	4.821722	-0.012785	1.716943
66.987909	854.476143	4.826726	-0.012879	1.723705
67.311741	862.658023	4.831731	-0.012945	1.730456
67.792611	870.811213	4.836736	-0.013039	1.737177
68.079665	878.990918	4.841741	-0.013098	1.743869
68.502220	887.142387	4.846746	-0.013182	1.750530
69.062939	895.294866	4.851750	-0.013292	1.757184
69.774684	903.398890	4.856755	-0.013429	1.763792
70.039605	911.582991	4.861760	-0.013484	1.770383
70.658707	919.733559	4.866765	-0.013604	1.776968
70.834192	927.925172	4.871770	-0.013642	1.783505
70.983103	936.121576	4.876774	-0.013675	1.790019
71.924010	944.244627	4.881779	-0.013856	1.796549
72.133550	952.386800	4.886784	-0.013900	1.802981
72.529508	960.543013	4.891789	-0.013979	1.809423
72.998290	968.671215	4.896794	-0.014071	1.815829
73.589285	976.779410	4.901798	-0.014186	1.822212
73.869935	984.953143	4.906803	-0.014244	1.828586
73.970953	993.140847	4.911808	-0.014268	1.834927
74.771653	1001.218834	4.916813	-0.014422	1.841244
75.020804	1009.378204	4.921818	-0.014474	1.847537
75.422796	1017.533849	4.926822	-0.014554	1.853824
75.977237	1025.649743	4.931827	-0.014662	1.860077
76.307180	1033.776361	4.936832	-0.014729	1.866291
76.349683	1042.003592	4.941837	-0.014742	1.872527
76.456916	1050.155858	4.946842	-0.014767	1.878693
76.907460	1058.219581	4.951846	-0.014856	1.884812
77.095547	1066.388837	4.956851	-0.014896	1.890960
77.668080	1074.457460	4.961856	-0.015008	1.897057
78.280384	1082.542552	4.966861	-0.015127	1.903150
78.829851	1090.661116	4.971866	-0.015235	1.909242
79.092063	1098.816423	4.976870	-0.015289	1.915309
79.381252	1106.943773	4.981875	-0.015348	1.921339
79.900395	1115.026533	4.986880	-0.015450	1.927343
80.507991	1123.148715	4.991885	-0.015568	1.933367
80.829315	1131.284480	4.996890	-0.015633	1.939351
81.225010	1139.390307	5.001894	-0.015712	1.945302
81.738418	1147.540013	5.006899	-0.015813	1.951280
81.917370	1155.695602	5.011904	-0.015851	1.957207
82.330678	1163.786238	5.016909	-0.015933	1.963095
82.491470	1171.909545	5.021914	-0.015969	1.968961
83.211582	1179.965664	5.026918	-0.016108	1.974822
83.558421	1188.076012	5.031923	-0.016178	1.980664
83.612960	1196.217784	5.036928	-0.016193	1.986480
83.782887	1204.369839	5.041933	-0.016230	1.992299
84.252297	1212.440154	5.046938	-0.016322	1.998074
84.511131	1220.542479	5.051942	-0.016376	2.003833
84.857122	1228.662971	5.056947	-0.016445	2.009597
85.068241	1236.779032	5.061952	-0.016490	2.015328
85.637180	1244.856382	5.066957	-0.016601	2.021052
86.107153	1252.939980	5.071962	-0.016693	2.026754
86.547808	1261.063615	5.076966	-0.016781	2.032465
87.007096	1269.164803	5.081971	-0.016871	2.038146
87.184584	1277.265254	5.086976	-0.016910	2.043782
87.497569	1285.386648	5.091981	-0.016973	2.049430
87.874818	1293.485490	5.096986	-0.017048	2.055054
88.253404	1301.565733	5.101990	-0.017124	2.060650
88.699507	1309.650186	5.106995	-0.017212	2.066240
88.584000	1317.817860	5.112000	-0.017196	2.071815
89.372241	1325.853497	5.117005	-0.017348	2.077376
89.661327	1333.939171	5.122010	-0.017407	2.082906
89.883378	1342.041581	5.127014	-0.017453	2.088426
90.352212	1350.145726	5.132019	-0.017546	2.093957
90.720315	1358.219365	5.137024	-0.017620	2.099443
91.074694	1366.312464	5.142029	-0.017691	2.104926
91.378084	1374.448761	5.147034	-0.017752	2.110419
91.736803	1382.583581	5.152038	-0.017824	2.115902
92.055511	1390.656651	5.157043	-0.017889	2.121325
92.331724	1398.707500	5.162048	-0.017945	2.126716
92.578671	1406.822954	5.167053	-0.017997	2.132133
93.057780	1414.886066	5.172058	-0.018091	2.137524
93.236125	1422.973807	5.177062	-0.018129	2.142889
93.686221	1431.060819	5.182067	-0.018218	2.148266
93.888580	1439.172046	5.187072	-0.018261	2.153621
94.282110	1447.241557	5.192077	-0.018340	2.158954
94.600707	1455.305014	5.197082	-0.018404	2.164263
94.655276	1463.425170	5.202086	-0.018419	2.169571
95.067353	1471.511778	5.207091	-0.018501	2.174877
95.310642	1479.577739	5.212096	-0.018552	2.180141
95.720927	1487.648621	5.217101	-0.018633	2.185411
95.933906	1495.770151	5.222106	-0.018678	2.190683
96.112009	1503.885585	5.227110	-0.018716	2.195936
96.695859	1511.911559	5.232115	-0.018830	2.201154
96.938367	1519.970122	5.237120	-0.018881	2.206351
97.182870	1528.080284	5.242125	-0.018931	2.211568
97.397191	1536.182978	5.247130	-0.018976	2.216766
97.792768	1544.225471	5.252134	-0.019055	2.221929
98.156648	1552.319178	5.257139	-0.019128	2.227110
98.173486	1560.429399	5.262144	-0.019136	2.232258
98.567994	1568.496406	5.267149	-0.019215	2.237401
99.067711	1576.538133	5.272154	-0.019313	2.242525
99.002709	1584.651359	5.277158	-0.019306	2.247632
99.382116	1592.745707	5.282163	-0.019382	2.252755
99.771101	1600.798147	5.287168	-0.019460	2.257841
100.009102	1608.883513	5.292173	-0.019509	2.262923
100.270525	1616.947705	5.297178	-0.019563	2.267982
100.780536	1625.063127	5.302182	-0.019663	2.273083
101.006044	1633.147277	5.307187	-0.019710	2.278129
101.186321	1641.186245	5.312192	-0.019749	2.283132
101.565574	1649.231190	5.317197	-0.019825	2.288144
102.160430	1657.271188	5.322202	-0.019941	2.293161
102.550985	1665.325874	5.327206	-0.020018	2.298158
102.708045	1673.422564	5.332211	-0.020053	2.303150
103.267001	1681.452032	5.337216	-0.020162	2.308125
103.692997	1689.540139	5.342221	-0.020247	2.313113
103.822459	1697.630804	5.347226	-0.020276	2.318067
104.201401	1705.676360	5.352230	-0.020351	2.323003
104.528989	1713.761201	5.357235	-0.020418	2.327949
104.670977	1721.863774	5.362240	-0.020449	2.332880
104.944579	1729.930879	5.367245	-0.020505	2.337789
105.461692	1737.961399	5.372250	-0.020607	2.342686
105.408008	1746.083877	5.377254	-0.020602	2.347582
105.863944	1754.160265	5.382259	-0.020692	2.352481
106.203892	1762.209140	5.387264	-0.020760	2.357343
106.484624	1770.262015	5.392269	-0.020818	2.362194
106.631729	1778.347563	5.397274	-0.020850	2.367043
106.952452	1786.402354	5.402278	-0.020915	2.371878
107.303087	1794.487356	5.407283	-0.020986	2.376723
107.486072	1802.531184	5.412288	-0.021025	2.381520
107.896885	1810.572947	5.417293	-0.021106	2.386325
108.139744	1818.667922	5.422298	-0.021157	2.391138
108.437933	1826.729684	5.427302	-0.021218	2.395926
108.969243	1834.757073	5.432307	-0.021322	2.400702
109.315902	1842.802845	5.437312	-0.021391	2.405466
109.787246	1850.863378	5.442317	-0.021484	2.410238
109.889532	1858.991893	5.447322	-0.021508	2.415012
110.226804	1867.030366	5.452326	-0.021576	2.419741
110.527481	1875.086700	5.457331	-0.021637	2.424469
110.850434	1883.138864	5.462336	-0.021703	2.429188
111.443828	1891.278367	5.467341	-0.021818	2.433968
112.086911	1899.272698	5.472346	-0.021943	2.438659
112.086886	1907.362118	5.477350	-0.021948	2.443346
112.454330	1915.418237	5.482355	-0.022022	2.448033
112.633496	1923.480919	5.487360	-0.022060	2.452701
113.001948	1931.538886	5.492365	-0.022134	2.457371
113.175617	1939.602325	5.497370	-0.022172	2.462020
113.340877	1947.654186	5.502374	-0.022208	2.466654
113.939420	1955.707318	5.507379	-0.022324	2.471312
113.808935	1963.803519	5.512384	-0.022305	2.475932
113.818700	1971.872705	5.517389	-0.022312	2.480538
114.314611	1979.886626	5.522394	-0.022409	2.485139
114.542262	1987.934854	5.527398	-0.022457	2.489732
114.917172	1996.015366	5.532403	-0.022532	2.494346
115.285751	2004.048467	5.537408	-0.022606	2.498923
115.583784	2012.100121	5.542413	-0.022666	2.503498
115.749139	2020.181035	5.547418	-0.022702	2.508071
116.071020	2028.253334	5.552422	-0.022767	2.512642
116.647936	2036.293597	5.557427	-0.022880	2.517205
117.004337	2044.312264	5.562432	-0.022951	2.521732
117.129802	2052.401372	5.567437	-0.022980	2.526273
117.499595	2060.459897	5.572442	-0.023054	2.530807
117.553059	2068.525386	5.577446	-0.023069	2.535314
117.939282	2076.573480	5.582451	-0.023146	2.539826
118.177116	2084.607289	5.587456	-0.023195	2.544313
118.620955	2092.657372	5.592461	-0.023283	2.548814
118.869310	2100.750453	5.597466	-0.023335	2.553318
119.268900	2108.765124	5.602470	-0.023414	2.557781
119.596538	2116.820407	5.607475	-0.023480	2.562254
119.719069	2124.883311	5.612480	-0.023508	2.566708
119.881232	2132.955590	5.617485	-0.023544	2.571163
120.198456	2141.018461	5.622490	-0.023608	2.575616
120.489264	2149.053810	5.627494	-0.023667	2.580044
120.826819	2157.093854	5.632499	-0.023735	2.584470
121.117069	2165.161256	5.637504	-0.023794	2.588900
121.281079	2173.394452	5.642509	-0.023830	2.593404
121.520252	2181.429062	5.647514	-0.023880	2.597798
121.594441	2189.426490	5.652518	-0.023899	2.602152
122.054210	2197.425862	5.657523	-0.023989	2.606527
122.402021	2205.454903	5.662528	-0.024059	2.610902
122.478341	2213.524425	5.667533	-0.024079	2.615274
122.596175	2221.578353	5.672538	-0.024106	2.619633
123.036224	2229.568215	5.677542	-0.024193	2.623971
123.361096	2237.635428	5.682547	-0.024258	2.628336
123.396741	2245.709232	5.687552	-0.024270	2.632679
123.733313	2253.749701	5.692557	-0.024338	2.637016
124.239487	2261.772832	5.697562	-0.024437	2.641347
124.256961	2269.821287	5.702566	-0.024446	2.645653
124.677772	2277.865874	5.707571	-0.024529	2.649977
124.926833	2285.934926	5.712576	-0.024581	2.654295
125.173255	2293.979438	5.717581	-0.024632	2.658593
125.464460	2302.024598	5.722586	-0.024691	2.662887
125.691190	2310.047789	5.727590	-0.024738	2.667158
126.071184	2318.126091	5.732595	-0.024814	2.671461
126.194060	2326.202801	5.737600	-0.024842	2.675740
126.547167	2334.197132	5.742605	-0.024913	2.679984
126.650570	2342.253553	5.747610	-0.024938	2.684237
127.039216	2350.269930	5.752614	-0.025015	2.688481
127.323975	2358.360505	5.757619	-0.025073	2.692750
127.699737	2366.367964	5.762624	-0.025148	2.696975
127.802152	2374.437198	5.767629	-0.025173	2.701208
127.998737	2382.498883	5.772634	-0.025214	2.705436
128.459258	2390.485404	5.777638	-0.025305	2.709635
128.540258	2398.613929	5.782643	-0.025325	2.713878
128.684013	2406.642087	5.787648	-0.025357	2.718066
129.063771	2414.641927	5.792653	-0.025433	2.722247
129.505412	2422.696893	5.797658	-0.025520	2.726455
129.701890	2430.725584	5.802662	-0.025562	2.730627
129.845848	2438.838136	5.807667	-0.025594	2.734832
130.064400	2446.862482	5.812672	-0.025640	2.738990
130.336078	2454.891655	5.817677	-0.025696	2.743148
130.488494	2462.960612	5.822682	-0.025729	2.747312
130.573143	2471.064486	5.827686	-0.025750	2.751484
130.768333	2479.165262	5.832691	-0.025792	2.755655
131.001807	2487.140450	5.837696	-0.025840	2.759757
131.584691	2495.118369	5.842701	-0.025954	2.763876
131.525415	2503.189893	5.847706	-0.025948	2.767998
131.344394	2511.276647	5.852710	-0.025919	2.772114
131.689867	2519.315055	5.857715	-0.025989	2.776230
132.279851	2527.278137	5.862720	-0.026104	2.780317
132.506925	2535.296751	5.867725	-0.026151	2.784404
132.628448	2543.389434	5.872730	-0.026179	2.788517
132.856895	2551.442262	5.877734	-0.026227	2.792610
132.954130	2559.512971	5.882739	-0.026250	2.796697
133.116705	2567.523664	5.887744	-0.026285	2.800753
133.341841	2575.545657	5.892749	-0.026332	2.804812
133.837770	2583.569290	5.897754	-0.026430	2.808881
133.950556	2591.632148	5.902758	-0.026456	2.812942
134.180803	2599.701949	5.907763	-0.026504	2.817008
134.626632	2607.720817	5.912768	-0.026592	2.821054
134.788464	2615.760249	5.917773	-0.026627	2.825089
134.797471	2623.832482	5.922778	-0.026634	2.829125
135.192395	2631.881621	5.927782	-0.026713	2.833167
135.650060	2639.917161	5.932787	-0.026803	2.837199
135.830819	2647.938136	5.937792	-0.026842	2.841202
135.899053	2655.975130	5.942797	-0.026860	2.845201
136.233285	2664.029214	5.947802	-0.026927	2.849218
136.127707	2672.084726	5.952806	-0.026913	2.853206
136.299547	2680.131495	5.957811	-0.026950	2.857199
136.598018	2688.140591	5.962816	-0.027010	2.861175
136.928467	2696.167526	5.967821	-0.027077	2.865155
137.188917	2704.220012	5.972826	-0.027131	2.869139
137.445167	2712.263368	5.977830	-0.027184	2.873113
138.051131	2720.282678	5.982835	-0.027302	2.877089
137.961957	2728.352266	5.987840	-0.027290	2.881045
138.244373	2736.341115	5.992845	-0.027348	2.884977
138.703637	2744.376212	5.997850	-0.027438	2.888936
138.734648	2752.464436	6.002854	-0.027449	2.892892
138.945484	2760.511167	6.007859	-0.027494	2.896832
139.214437	2768.536908	6.012864	-0.027549	2.900759
139.599718	2776.530659	6.017869	-0.027626	2.904672
139.885373	2784.601013	6.022874	-0.027684	2.908611
140.150657	2792.709164	6.027878	-0.027739	2.912562
140.427365	2800.783410	6.032883	-0.027795	2.916492
140.592357	2808.777099	6.037888	-0.027831	2.920372
140.709022	2816.760970	6.042893	-0.027858	2.924239
141.110161	2824.789692	6.047898	-0.027938	2.928138
141.297067	2832.839776	6.052902	-0.027978	2.932031
141.434947	2840.903414	6.057907	-0.028009	2.935922
141.851424	2848.902707	6.062912	-0.028091	2.939792
142.219330	2856.908940	6.067917	-0.028165	2.943657
142.299327	2864.990974	6.072922	-0.028185	2.947539
142.576225	2873.040885	6.077926	-0.028242	2.951410
143.094215	2881.071561	6.082931	-0.028343	2.955279
143.116298	2889.112909	6.087936	-0.028352	2.959123
143.200361	2897.141041	6.092941	-0.028373	2.962959
143.339790	2905.196620	6.097946	-0.028404	2.966805
143.521912	2913.217466	6.102950	-0.028443	2.970633
143.590536	2921.300337	6.107955	-0.028461	2.974479
144.075954	2929.276797	6.112960	-0.028557	2.978290
144.354419	2937.305577	6.117965	-0.028614	2.982111
144.557563	2945.364702	6.122970	-0.028657	2.985938
144.821067	2953.378985	6.127974	-0.028711	2.989742
145.199792	2961.464150	6.132979	-0.028786	2.993579
145.352612	2969.481169	6.137984	-0.028820	2.997369
145.465482	2977.519936	6.142989	-0.028846	3.001162
145.820581	2985.532763	6.147994	-0.028917	3.004950
146.170407	2993.543819	6.152998	-0.028988	3.008732
146.416294	3001.632644	6.158003	-0.029039	3.012540
146.685771	3009.669387	6.163008	-0.029094	3.016321
146.777784	3017.690233	6.168013	-0.029116	3.020080
146.990336	3025.718553	6.173018	-0.029161	3.023844
147.089247	3033.752124	6.178022	-0.029184	3.027601
147.616325	3041.787318	6.183027	-0.029288	3.031374
147.907668	3049.860657	6.188032	-0.029347	3.035149
147.933156	3057.891207	6.193037	-0.029357	3.038886
148.187797	3065.915333	6.198042	-0.029409	3.042627
148.436276	3073.925877	6.203046	-0.029461	3.046357
148.659760	3081.993431	6.208051	-0.029508	3.050107
148.783158	3090.029383	6.213056	-0.029536	3.053833
149.173756	3098.053168	6.218061	-0.029614	3.057561
149.295327	3106.109813	6.223066	-0.029641	3.061288
149.475945	3114.103928	6.228070	-0.029680	3.064984
149.952876	3122.132440	6.233075	-0.029774	3.068705
150.293273	3130.221535	6.238080	-0.029843	3.072443
150.268409	3138.311618	6.243085	-0.029843	3.076159
150.578374	3146.288992	6.248090	-0.029906	3.079836
150.888142	3154.274038	6.253094	-0.029969	3.083511
150.978655	3162.323026	6.258099	-0.029991	3.087201
151.077268	3170.378147	6.263104	-0.030014	3.090889
151.301585	3178.387195	6.268109	-0.030061	3.094558
151.689325	3186.415442	6.273114	-0.030138	3.098239
151.806888	3194.445613	6.278118	-0.030165	3.101904
151.910387	3202.489503	6.283123	-0.030190	3.105570
151.977975	3210.520440	6.288128	-0.030207	3.109225
152.140674	3218.566504	6.293133	-0.030243	3.112886
152.508588	3226.612014	6.298138	-0.030316	3.116552
152.584019	3234.602500	6.303142	-0.030336	3.120175
152.959181	3242.620204	6.308147	-0.030411	3.123820
153.018533	3250.664928	6.313152	-0.030427	3.127459
153.220704	3258.725006	6.318157	-0.030470	3.131106
153.447822	3266.798366	6.323162	-0.030517	3.134757
153.624494	3274.793287	6.328166	-0.030555	3.138366
153.917687	3282.809664	6.333171	-0.030615	3.141985
154.195131	3290.841849	6.338176	-0.030672	3.145607
154.299163	3298.860741	6.343181	-0.030696	3.149210
154.842494	3306.937936	6.348186	-0.030802	3.152855
155.087305	3314.956202	6.353190	-0.030853	3.156456
155.250414	3322.971450	6.358195	-0.030888	3.160049
155.609786	3330.968458	6.363200	-0.030961	3.163637
155.823401	3339.003557	6.368205	-0.031005	3.167232
156.051197	3347.059141	6.373210	-0.031053	3.170833
156.137452	3355.108198	6.378214	-0.031074	3.174420
156.428253	3363.130553	6.383219	-0.031133	3.178000
156.797822	3371.167191	6.388224	-0.031207	3.181586
156.814817	3379.187778	6.393229	-0.031216	3.185146
157.157572	3387.246774	6.398234	-0.031285	3.188733
157.325691	3395.278789	6.403238	-0.031321	3.192296
157.415748	3403.330844	6.408243	-0.031343	3.195861
157.655735	3411.309081	6.413248	-0.031393	3.199395
158.052469	3419.312529	6.418253	-0.031472	3.202943
158.341590	3427.365728	6.423258	-0.031531	3.206505
158.423808	3435.415670	6.428262	-0.031551	3.210052
158.617832	3443.486742	6.433267	-0.031592	3.213610
158.720044	3451.498000	6.438272	-0.031617	3.217133
158.937856	3459.512927	6.443277	-0.031662	3.220659
159.401540	3467.520105	6.448282	-0.031754	3.224188
159.533421	3475.550224	6.453286	-0.031783	3.227709
159.811271	3483.616260	6.458291	-0.031840	3.231248
160.124420	3491.694428	6.463296	-0.031904	3.234790
160.417345	3499.663955	6.468301	-0.031963	3.238280
160.679067	3507.701018	6.473306	-0.032017	3.241794
160.732754	3515.702361	6.478310	-0.032032	3.245281
161.001486	3523.727652	6.483315	-0.032087	3.248782
161.269523	3531.760367	6.488320	-0.032142	3.252283
161.075816	3539.841494	6.493325	-0.032112	3.255783
161.398082	3547.844936	6.498330	-0.032177	3.259266
161.566789	3555.843769	6.503334	-0.032213	3.262737
161.908833	3563.888784	6.508339	-0.032282	3.266231
162.024385	3571.906159	6.513344	-0.032309	3.269701
162.207324	3579.981687	6.518349	-0.032348	3.273194
162.546669	3588.027101	6.523354	-0.032416	3.276677
162.557618	3596.016037	6.528358	-0.032423	3.280119
162.855290	3604.028807	6.533363	-0.032484	3.283579
163.185032	3612.044377	6.538368	-0.032550	3.287037
163.243846	3620.085689	6.543373	-0.032566	3.290493
163.540299	3628.154904	6.548378	-0.032627	3.293966
163.648912	3636.167266	6.553382	-0.032652	3.297403
163.927402	3644.181599	6.558387	-0.032709	3.300845
164.345898	3652.187551	6.563392	-0.032792	3.304284
164.401096	3660.243934	6.568397	-0.032807	3.307728
164.906848	3668.286984	6.573402	-0.032907	3.311179
164.825634	3676.331400	6.578406	-0.032897	3.314605
164.982703	3684.350543	6.583411	-0.032931	3.318026
165.216792	3692.363162	6.588416	-0.032980	3.321443
165.396809	3700.341876	6.593421	-0.033018	3.324841
165.526089	3708.400263	6.598426	-0.033048	3.328267
165.706336	3716.444135	6.603430	-0.033086	3.331684
166.170511	3724.468552	6.608435	-0.033178	3.335101
166.287459	3732.498548	6.613440	-0.033205	3.338504
166.437913	3740.517624	6.618445	-0.033238	3.341900
166.798662	3748.559187	6.623450	-0.033310	3.345309
167.027066	3756.556949	6.628454	-0.033358	3.348692
167.165223	3764.627791	6.633459	-0.033389	3.352099
167.262133	3772.686741	6.638464	-0.033412	3.355495
167.518138	3780.654054	6.643469	-0.033465	3.358856
167.613033	3788.712462	6.648474	-0.033488	3.362245
167.847126	3796.716511	6.653478	-0.033536	3.365614
168.157178	3804.736345	6.658483	-0.033599	3.368988
168.162320	3812.812786	6.663488	-0.033605	3.372372
168.389485	3820.838869	6.668493	-0.033653	3.375739
168.830283	3828.839228	6.673498	-0.033740	3.379099
168.837034	3836.878603	6.678502	-0.033746	3.382457
169.221644	3844.876780	6.683507	-0.033823	3.385808
169.327115	3852.911135	6.688512	-0.033848	3.389161
169.616973	3861.000977	6.693517	-0.033907	3.392540
169.942824	3869.065220	6.698522	-0.033973	3.395906
170.100842	3877.008145	6.703526	-0.034007	3.399212
170.406462	3885.033052	6.708531	-0.034069	3.402555
170.698972	3893.053541	6.713536	-0.034129	3.405892
170.779410	3901.054470	6.718541	-0.034149	3.409210
171.019957	3909.141993	6.723546	-0.034199	3.412566
171.117654	3917.163333	6.728550	-0.034222	3.415886
171.232882	3925.153279	6.733555	-0.034249	3.419191
171.406161	3933.204499	6.738560	-0.034286	3.422520
171.777921	3941.187469	6.743565	-0.034360	3.425825
172.100996	3949.225544	6.748570	-0.034426	3.429147
172.057200	3957.305416	6.753574	-0.034423	3.432471
172.340658	3965.329900	6.758579	-0.034480	3.435779
172.554272	3973.346658	6.763584	-0.034525	3.439079
172.433492	3981.370254	6.768589	-0.034508	3.442368
173.022845	3989.378908	6.773594	-0.034623	3.445670
173.186836	3997.374280	6.778598	-0.034658	3.448950
173.290944	4005.434855	6.783603	-0.034683	3.452252
173.511361	4013.491541	6.788608	-0.034729	3.455552
173.735502	4021.472373	6.793613	-0.034776	3.458819
174.056749	4029.527337	6.798618	-0.034841	3.462116
174.001898	4037.532082	6.803622	-0.034836	3.465377
174.468953	4045.567917	6.808627	-0.034928	3.468664
174.487519	4053.648821	6.813632	-0.034937	3.471952
174.562493	4061.687582	6.818637	-0.034956	3.475222
174.920721	4069.674605	6.823642	-0.035027	3.478477
175.224522	4077.646632	6.828646	-0.035089	3.481720
175.222611	4085.657263	6.833651	-0.035094	3.484967
175.294187	4093.723592	6.838656	-0.035112	3.488235
175.576378	4101.747040	6.843661	-0.035170	3.491490
175.890280	4109.770996	6.848666	-0.035234	3.494743
176.069276	4117.768236	6.853670	-0.035272	3.497978
176.520912	4125.808275	6.858675	-0.035361	3.501235
176.696352	4133.810806	6.863680	-0.035399	3.504466
176.633061	4141.857910	6.868685	-0.035392	3.507704
176.919757	4149.930431	6.873690	-0.035451	3.510960
177.172541	4157.938590	6.878694	-0.035503	3.514186
177.167391	4165.953826	6.883699	-0.035507	3.517405
177.334734	4173.998223	6.888704	-0.035543	3.520637
177.569471	4181.956881	6.893709	-0.035592	3.523834
177.816353	4190.019458	6.898714	-0.035643	3.527070
177.779027	4198.051059	6.903718	-0.035642	3.530282
178.141879	4206.097896	6.908723	-0.035714	3.533509
178.565146	4214.107017	6.913728	-0.035798	3.536720
178.450072	4222.117276	6.918733	-0.035782	3.539912
178.849097	4230.158706	6.923738	-0.035861	3.543129
179.025669	4238.185905	6.928742	-0.035899	3.546331
179.152484	4246.203763	6.933747	-0.035928	3.549525
179.373415	4254.338168	6.938752	-0.035974	3.552765
179.461037	4262.352407	6.943757	-0.035996	3.555950
179.448828	4270.341151	6.948762	-0.035999	3.559120
179.455592	4278.320641	6.953766	-0.036005	3.562283
179.798270	4286.315522	6.958771	-0.036074	3.565460
179.939827	4294.365674	6.963776	-0.036105	3.568650
179.964821	4302.387432	6.968781	-0.036115	3.571822
180.445901	4310.424797	6.973786	-0.036210	3.575011
180.934457	4318.395417	6.978790	-0.036306	3.578171
180.953388	4326.428164	6.983795	-0.036314	3.581339
181.129911	4334.447059	6.988800	-0.036352	3.584503
181.522340	4342.445557	6.993805	-0.036431	3.587662
181.652220	4350.545743	6.998810	-0.036460	3.590851
181.950680	4358.539276	7.003814	-0.036521	3.594000
182.087776	4366.580220	7.008819	-0.036551	3.597161
182.450660	4374.573076	7.013824	-0.036624	3.600306
182.440350	4382.565534	7.018829	-0.036627	3.603438
182.662214	4390.635326	7.023834	-0.036674	3.606603
182.941009	4398.626022	7.028838	-0.036731	3.609737
183.169772	4406.652119	7.033843	-0.036778	3.612880
183.336894	4414.740871	7.038848	-0.036815	3.616043
183.420671	4422.712184	7.043853	-0.036835	3.619156
183.678802	4430.742225	7.048858	-0.036888	3.622293
183.674697	4438.776914	7.053862	-0.036893	3.625422
183.894555	4446.806077	7.058867	-0.036939	3.628553
184.129035	4454.860539	7.063872	-0.036988	3.631691
184.113967	4462.883979	7.068877	-0.036990	3.634807
184.482289	4470.906190	7.073882	-0.037064	3.637930
184.664722	4478.905653	7.078886	-0.037103	3.641038
184.906813	4486.862775	7.083891	-0.037153	3.644127
185.082486	4494.941064	7.088896	-0.037191	3.647259
185.118725	4502.976201	7.093901	-0.037203	3.650368
185.362634	4511.038744	7.098906	-0.037253	3.653490
185.474097	4519.075282	7.103910	-0.037279	3.656596
185.699567	4527.042944	7.108915	-0.037326	3.659676
185.990645	4535.083464	7.113920	-0.037386	3.662783
185.938497	4543.090927	7.118925	-0.037381	3.665866
186.147902	4551.119925	7.123930	-0.037425	3.668961
186.365761	4559.173918	7.128934	-0.037471	3.672063
186.444547	4567.175053	7.133939	-0.037490	3.675139
186.730902	4575.217865	7.138944	-0.037549	3.678234
186.758453	4583.235175	7.143949	-0.037559	3.681309
187.050307	4591.200057	7.148954	-0.037619	3.684369
187.106286	4599.242812	7.153958	-0.037634	3.687450
187.548998	4607.246338	7.158963	-0.037722	3.690523
187.929292	4615.321322	7.163968	-0.037798	3.693619
188.056466	4623.329939	7.168973	-0.037826	3.696680
188.284128	4631.337853	7.173978	-0.037874	3.699742
188.619604	4639.361845	7.178982	-0.037942	3.702809
188.744359	4647.369484	7.183987	-0.037970	3.705863
188.859486	4655.429545	7.188992	-0.037996	3.708934
189.215153	4663.452021	7.193997	-0.038068	3.711994
189.517766	4671.557858	7.199002	-0.038129	3.715081
189.577072	4679.540644	7.204006	-0.038145	3.718114
189.929359	4687.518584	7.209011	-0.038216	3.721149
190.137885	4695.476969	7.214016	-0.038260	3.724171
190.197571	4703.512434	7.219021	-0.038276	3.727216
190.462719	4711.524929	7.224026	-0.038331	3.730254
190.443241	4719.584429	7.229030	-0.038332	3.733301
190.781060	4727.623794	7.234035	-0.038400	3.736347
190.940594	4735.638916	7.239040	-0.038435	3.739377
190.931297	4743.648864	7.244045	-0.038438	3.742398
191.459616	4751.647364	7.249050	-0.038542	3.745425
191.510052	4759.717241	7.254054	-0.038557	3.748465
191.643765	4767.740375	7.259059	-0.038587	3.751487
191.556291	4775.810349	7.264064	-0.038575	3.754519
191.724219	4783.796196	7.269069	-0.038612	3.757523
191.986673	4791.818464	7.274074	-0.038666	3.760541
192.120486	4799.809404	7.279078	-0.038696	3.763541
192.446200	4807.841698	7.284083	-0.038762	3.766559
192.751434	4815.845970	7.289088	-0.038823	3.769563
192.739379	4823.884431	7.294093	-0.038826	3.772570
193.002494	4831.953544	7.299098	-0.038880	3.775593
193.070054	4839.947435	7.304102	-0.038898	3.778581
193.011785	4847.989582	7.309107	-0.038892	3.781581
193.466834	4855.971240	7.314112	-0.038982	3.784568
193.729504	4863.991886	7.319117	-0.039036	3.787563
193.934463	4872.052642	7.324122	-0.039080	3.790570
193.813907	4880.094777	7.329126	-0.039062	3.793559
193.944919	4888.114847	7.334131	-0.039092	3.796544
194.275459	4896.078211	7.339136	-0.039158	3.799509
194.254547	4904.113252	7.344141	-0.039160	3.802492
194.664744	4912.098962	7.349146	-0.039241	3.805462
194.830369	4920.129012	7.354150	-0.039277	3.808442
194.826326	4928.187137	7.359155	-0.039281	3.811426
195.002401	4936.195529	7.364160	-0.039319	3.814393
195.403554	4944.182836	7.369165	-0.039399	3.817355
195.633199	4952.230392	7.374170	-0.039447	3.820333
195.823319	4960.207930	7.379174	-0.039488	3.823282
195.962225	4968.274242	7.384179	-0.039519	3.826261
196.130162	4976.280002	7.389184	-0.039555	3.829215
196.202703	4984.347491	7.394189	-0.039574	3.832188
196.521545	4992.341101	7.399194	-0.039638	3.835136
196.618974	5000.367977	7.404198	-0.039661	3.838090
196.758996	5008.369782	7.409203	-0.039692	3.841033
197.044365	5016.372176	7.414208	-0.039751	3.843977
197.223260	5024.420850	7.419213	-0.039789	3.846934
197.373367	5032.419474	7.424218	-0.039822	3.849869
197.415840	5040.492501	7.429222	-0.039835	3.852827
197.489482	5048.500062	7.434227	-0.039854	3.855760
197.696436	5056.507249	7.439232	-0.039898	3.858692
197.657607	5064.556370	7.444237	-0.039896	3.861633
197.955891	5072.506752	7.449242	-0.039956	3.864543
198.227847	5080.591368	7.454246	-0.040012	3.867498
198.403371	5088.584760	7.459251	-0.040050	3.870416
198.701002	5096.845086	7.464256	-0.040111	3.873432
198.731661	5104.857908	7.469261	-0.040121	3.876350
198.877691	5112.767553	7.474266	-0.040154	3.879230
199.149345	5120.747712	7.479270	-0.040209	3.882136
199.111328	5128.703246	7.484275	-0.040207	3.885025
199.420322	5136.748593	7.489280	-0.040270	3.887952
199.330428	5144.742959	7.494285	-0.040258	3.890850
199.751512	5152.784302	7.499290	-0.040342	3.893772
199.918823	5160.875432	7.504294	-0.040378	3.896706
200.014771	5168.827180	7.509299	-0.040401	3.899585
199.973326	5176.856815	7.514304	-0.040398	3.902488
200.202917	5184.844584	7.519309	-0.040446	3.905378
200.349488	5192.872960	7.524314	-0.040479	3.908280
200.376740	5200.904889	7.529318	-0.040489	3.911178
200.658611	5208.903685	7.534323	-0.040546	3.914068
200.957921	5216.950101	7.539328	-0.040607	3.916972
201.069230	5224.910737	7.544333	-0.040633	3.919840
201.057239	5232.964279	7.549338	-0.040636	3.922737
201.509592	5240.968063	7.554342	-0.040725	3.925622
201.691092	5248.968154	7.559347	-0.040764	3.928499
201.755121	5257.054070	7.564352	-0.040781	3.931403
201.847710	5265.074904	7.569357	-0.040804	3.934281
202.110246	5273.111464	7.574362	-0.040858	3.937166
202.192169	5281.069721	7.579366	-0.040878	3.940018
202.167121	5289.100177	7.584371	-0.040879	3.942891
202.450742	5297.122988	7.589376	-0.040936	3.945765
202.527050	5305.117403	7.594381	-0.040956	3.948623
202.710964	5313.198962	7.599386	-0.040995	3.951513
203.110537	5321.255865	7.604390	-0.041075	3.954395
203.286436	5329.224590	7.609395	-0.041113	3.957239
203.439307	5337.219529	7.614400	-0.041146	3.960090
203.543443	5345.220019	7.619405	-0.041171	3.962941
203.849639	5353.226271	7.624410	-0.041233	3.965794
203.903136	5361.237339	7.629414	-0.041248	3.968644
203.920449	5369.268224	7.634419	-0.041256	3.971497
204.397739	5377.295390	7.639424	-0.041350	3.974355
204.552312	5385.346434	7.644429	-0.041384	3.977214
204.651461	5393.334592	7.649434	-0.041408	3.980047
204.958215	5401.361080	7.654438	-0.041470	3.982896
205.277168	5409.353181	7.659443	-0.041534	3.985730
205.386349	5417.431491	7.664448	-0.041560	3.988590
205.267115	5425.444055	7.669453	-0.041543	3.991420
205.693128	5433.510521	7.674458	-0.041627	3.994277
205.789902	5441.552047	7.679462	-0.041650	3.997117
205.948224	5449.505332	7.684467	-0.041685	3.999925
206.038659	5457.535592	7.689472	-0.041707	4.002757
206.101423	5465.518752	7.694477	-0.041724	4.005569
206.392718	5473.549597	7.699482	-0.041783	4.008401
206.576502	5481.615941	7.704486	-0.041822	4.011241
206.603640	5489.657772	7.709491	-0.041833	4.014068
206.702223	5497.691440	7.714496	-0.041856	4.016891
206.944627	5505.648798	7.719501	-0.041906	4.019688
207.227264	5513.698185	7.724506	-0.041964	4.022515
207.274071	5521.712041	7.729510	-0.041978	4.025325
207.326147	5529.732185	7.734515	-0.041993	4.028135
207.699136	5537.760934	7.739520	-0.042067	4.030950
207.842788	5545.859875	7.744525	-0.042099	4.033785
207.944325	5553.884190	7.749530	-0.042123	4.036591
208.073553	5561.800278	7.754534	-0.042152	4.039358
208.475935	5569.784440	7.759539	-0.042232	4.042151
208.696552	5577.821438	7.764544	-0.042278	4.044957
208.756195	5585.827928	7.769549	-0.042295	4.047748
208.985487	5593.852546	7.774554	-0.042343	4.050547
209.135026	5601.931032	7.779558	-0.042376	4.053360
209.216455	5609.921969	7.784563	-0.042396	4.056141
209.470055	5617.884309	7.789568	-0.042448	4.058912
209.759702	5625.937032	7.794573	-0.042507	4.061713
210.001296	5633.920039	7.799578	-0.042557	4.064487
210.475877	5641.957579	7.804582	-0.042651	4.067282
210.676476	5649.939052	7.809587	-0.042693	4.070051
210.707774	5658.031213	7.814592	-0.042704	4.072854
210.608919	5666.048513	7.819597	-0.042691	4.075628
210.966949	5674.005904	7.824602	-0.042763	4.078385
211.257055	5682.054680	7.829606	-0.042822	4.081171
211.285957	5690.015516	7.834611	-0.042832	4.083921
211.491550	5698.119494	7.839616	-0.042876	4.086722
211.494188	5706.061485	7.844621	-0.042881	4.089461
211.662568	5714.142732	7.849626	-0.042918	4.092249
211.868101	5722.189131	7.854630	-0.042961	4.095024
211.955912	5730.183056	7.859635	-0.042983	4.097777
212.332624	5738.195737	7.864640	-0.043058	4.100538
212.326805	5746.185100	7.869645	-0.043062	4.103284
212.451401	5754.212098	7.874650	-0.043090	4.106044
212.733280	5762.234923	7.879654	-0.043148	4.108802
212.714954	5770.301951	7.884659	-0.043149	4.111569
213.055807	5778.361780	7.889664	-0.043218	4.114337
213.075214	5786.385463	7.894669	-0.043227	4.117086
213.074728	5794.325875	7.899674	-0.043232	4.119804
213.267688	5802.390318	7.904678	-0.043273	4.122566
213.450193	5810.339163	7.909683	-0.043312	4.125286
213.856053	5818.373787	7.914688	-0.043393	4.128037
213.800404	5826.385995	7.919693	-0.043387	4.130772
213.961031	5834.447802	7.924698	-0.043422	4.133525
214.122939	5842.514096	7.929702	-0.043458	4.136278
214.255986	5850.476904	7.934707	-0.043488	4.138993
214.477250	5858.523463	7.939712	-0.043534	4.141736
214.569124	5866.464434	7.944717	-0.043556	4.144440
214.900047	5874.527979	7.949722	-0.043623	4.147186
214.945098	5882.590530	7.954726	-0.043636	4.149927
215.137509	5890.583402	7.959731	-0.043677	4.152644
215.411334	5898.650530	7.964736	-0.043733	4.155385
215.412841	5906.627566	7.969741	-0.043739	4.158091
215.596366	5914.610915	7.974746	-0.043778	4.160799
215.662224	5922.608182	7.979750	-0.043795	4.163509
215.671956	5930.671643	7.984755	-0.043802	4.166239
215.924499	5938.692499	7.989760	-0.043855	4.168956
216.220109	5946.703393	7.994765	-0.043915	4.171667
216.295843	5954.734373	7.999770	-0.043934	4.174382
216.445876	5962.757976	8.004774	-0.043967	4.177093
216.596968	5970.710930	8.009779	-0.044000	4.179778
216.828659	5978.795153	8.014784	-0.044048	4.182506
216.945423	5986.757839	8.019789	-0.044075	4.185191
217.037651	5994.799749	8.024794	-0.044098	4.187900
217.216534	6002.836693	8.029798	-0.044136	4.190607
217.215724	6010.910675	8.034803	-0.044141	4.193323
217.464442	6018.957787	8.039808	-0.044192	4.196030
217.562373	6026.867151	8.044813	-0.044216	4.198688
217.603112	6034.911761	8.049818	-0.044228	4.201389
217.872928	6042.919028	8.054822	-0.044284	4.204078
218.101259	6050.907678	8.059827	-0.044331	4.206758
218.258924	6058.921417	8.064832	-0.044366	4.209445
218.233841	6066.976740	8.069837	-0.044366	4.212141
218.343371	6074.948180	8.074842	-0.044392	4.214810
218.781464	6082.991346	8.079846	-0.044479	4.217504
218.521221	6090.980505	8.084851	-0.044435	4.220171
218.940069	6099.035653	8.089856	-0.044518	4.222865
219.197333	6107.013904	8.094861	-0.044571	4.225530
219.357311	6115.077894	8.099866	-0.044606	4.228222
219.441782	6123.112769	8.104870	-0.044627	4.230901
219.741477	6131.131505	8.109875	-0.044688	4.233575
220.021355	6139.168209	8.114880	-0.044745	4.236253
219.937387	6147.108875	8.119885	-0.044735	4.238894
220.017401	6155.144653	8.124890	-0.044755	4.241566
220.259236	6163.100115	8.129894	-0.044805	4.244212
220.350543	6171.173045	8.134899	-0.044827	4.246893
220.575920	6179.152319	8.139904	-0.044874	4.249543
220.622440	6187.236754	8.144909	-0.044888	4.252225
220.816926	6195.239314	8.149914	-0.044929	4.254879
220.886530	6203.307894	8.154918	-0.044947	4.257552
221.058247	6211.251433	8.159923	-0.044984	4.260183
221.338614	6219.313145	8.164928	-0.045042	4.262852
221.650794	6227.282822	8.169933	-0.045105	4.265489
221.628156	6235.358168	8.174938	-0.045106	4.268157
221.969199	6243.367474	8.179942	-0.045174	4.270804
222.115072	6251.434337	8.184947	-0.045207	4.273468
222.167293	6259.476537	8.189952	-0.045222	4.276120
222.356218	6267.414093	8.194957	-0.045262	4.278738
222.517917	6275.450215	8.199962	-0.045297	4.281386
222.648417	6283.425763	8.204966	-0.045326	4.284012
222.725632	6291.445587	8.209971	-0.045346	4.286651
223.225939	6299.483537	8.214976	-0.045444	4.289297
223.293479	6307.527916	8.219981	-0.045462	4.291940
223.142589	6315.546535	8.224986	-0.045439	4.294572
223.243843	6323.614288	8.229990	-0.045463	4.297220
223.389509	6331.530759	8.234995	-0.045495	4.299817
223.580783	6339.605354	8.240000	-0.045536	4.302465
223.728472	6347.572582	8.245005	-0.045568	4.305076
224.098287	6355.602419	8.250010	-0.045642	4.307707
224.139565	6363.657455	8.255014	-0.045655	4.310342
224.101526	6371.686814	8.260019	-0.045653	4.312967
224.340954	6379.693614	8.265024	-0.045703	4.315585
224.486865	6387.667352	8.270029	-0.045735	4.318189
224.475937	6395.638051	8.275034	-0.045738	4.320790
224.876875	6403.735466	8.280038	-0.045818	4.323434
225.050331	6411.706067	8.285043	-0.045855	4.326033
225.112400	6419.719479	8.290048	-0.045872	4.328644
225.243447	6427.770784	8.295053	-0.045902	4.331266
225.472118	6435.789386	8.300058	-0.045949	4.333876
225.784592	6443.832247	8.305062	-0.046013	4.336493
225.771199	6451.811134	8.310067	-0.046015	4.339086
225.947711	6459.829242	8.315072	-0.046053	4.341691
226.175009	6467.813650	8.320077	-0.046101	4.344283
226.444834	6475.855962	8.325082	-0.046156	4.346894
226.605071	6483.883321	8.330086	-0.046191	4.349497
226.710722	6491.884862	8.335091	-0.046216	4.352090
226.962682	6500.038746	8.340096	-0.046268	4.354731
227.013868	6508.025077	8.345101	-0.046283	4.357316
227.222386	6515.948356	8.350106	-0.046326	4.359879
227.355563	6523.960003	8.355110	-0.046356	4.362469
227.471844	6531.918786	8.360115	-0.046383	4.365040
227.758786	6539.980620	8.365120	-0.046442	4.367644
227.957776	6547.946447	8.370125	-0.046484	4.370215
227.931849	6555.995872	8.375130	-0.046484	4.372810
228.137825	6564.076769	8.380134	-0.046528	4.375415
228.180354	6572.058909	8.385139	-0.046541	4.377986
228.454840	6580.101694	8.390144	-0.046597	4.380576
228.344933	6588.102894	8.395149	-0.046581	4.383149
228.420194	6596.052018	8.400154	-0.046601	4.385705
228.502858	6604.101922	8.405158	-0.046621	4.388291
228.663037	6612.130945	8.410163	-0.046656	4.390870
229.092162	6620.176658	8.415168	-0.046741	4.393454
229.101777	6628.228610	8.420173	-0.046748	4.396036
229.163623	6636.178217	8.425178	-0.046765	4.398584
229.227728	6644.230898	8.430182	-0.046782	4.401164
229.368366	6652.176840	8.435187	-0.046813	4.403708
229.470480	6660.238367	8.440192	-0.046837	4.406288
229.507124	6668.240284	8.445197	-0.046849	4.408847
229.738008	6676.277985	8.450202	-0.046897	4.411417
229.911301	6684.347778	8.455206	-0.046934	4.413995
229.866143	6692.360204	8.460211	-0.046931	4.416552
230.290809	6700.362230	8.465216	-0.047015	4.419107
230.324882	6708.387708	8.470221	-0.047027	4.421666
230.471577	6716.331884	8.475226	-0.047059	4.424198
230.702921	6724.402993	8.480230	-0.047107	4.426769
230.837241	6732.409656	8.485235	-0.047138	4.429318
231.061648	6740.471736	8.490240	-0.047184	4.431883
231.487996	6748.502322	8.495245	-0.047269	4.434438
231.529237	6756.515571	8.500250	-0.047282	4.436984
231.863034	6764.469423	8.505254	-0.047349	4.439511
231.980611	6772.491895	8.510259	-0.047376	4.442057
232.286581	6780.469239	8.515264	-0.047438	4.444588
232.277168	6788.560839	8.520269	-0.047441	4.447153
232.386642	6796.510655	8.525274	-0.047467	4.449672
232.593344	6804.623575	8.530278	-0.047511	4.452241
232.804894	6812.586259	8.535283	-0.047555	4.454762
233.092636	6820.621724	8.540288	-0.047614	4.457304
233.071155	6828.636032	8.545293	-0.047615	4.459837
233.399449	6836.620044	8.550298	-0.047681	4.462360
233.703345	6844.591193	8.555302	-0.047743	4.464878
233.668137	6852.612483	8.560307	-0.047741	4.467408
234.048352	6860.694967	8.565312	-0.047817	4.469958
234.164455	6868.749520	8.570317	-0.047844	4.472497
234.060655	6876.719915	8.575322	-0.047830	4.475007
234.390123	6884.757510	8.580327	-0.047896	4.477539
234.598612	6892.711746	8.585331	-0.047940	4.480042
234.845368	6900.750565	8.590336	-0.047991	4.482570
234.867728	6908.731740	8.595341	-0.048001	4.485078
234.884562	6916.787054	8.600346	-0.048009	4.487609
235.004446	6924.838946	8.605351	-0.048036	4.490136
235.183325	6932.862012	8.610355	-0.048075	4.492654
235.493022	6940.837620	8.615360	-0.048137	4.495156
235.591229	6948.892512	8.620365	-0.048161	4.497680
235.725232	6956.847952	8.625370	-0.048191	4.500172
235.653833	6964.887507	8.630375	-0.048183	4.502688
235.748413	6972.856226	8.635379	-0.048205	4.505182
235.990332	6980.922034	8.640384	-0.048256	4.507704
235.871821	6988.926507	8.645389	-0.048239	4.510205
236.244837	6996.977385	8.650394	-0.048313	4.512721
236.637952	7005.041756	8.655399	-0.048392	4.515239
236.682048	7012.980354	8.660403	-0.048405	4.517716
236.691391	7020.960653	8.665408	-0.048412	4.520204
236.941758	7029.000711	8.670413	-0.048463	4.522710
237.190839	7036.974152	8.675418	-0.048515	4.525194
237.220635	7045.038881	8.680423	-0.048526	4.527704
237.331939	7052.997135	8.685427	-0.048551	4.530180
237.576554	7061.071408	8.690432	-0.048602	4.532691
237.466229	7069.087203	8.695437	-0.048587	4.535182
237.622079	7077.132872	8.700442	-0.048621	4.537681
237.764491	7085.110692	8.705447	-0.048652	4.540158
237.917313	7093.100923	8.710451	-0.048686	4.542637
237.990556	7101.087975	8.715456	-0.048705	4.545114
238.383696	7109.145207	8.720461	-0.048783	4.547611
238.554103	7117.111398	8.725466	-0.048820	4.550079
238.625526	7125.243893	8.730471	-0.048838	4.552596
238.696584	7133.211352	8.735475	-0.048857	4.555062
238.892775	7141.273478	8.740480	-0.048898	4.557555
239.002010	7149.224283	8.745485	-0.048924	4.560012
238.997171	7157.251692	8.750490	-0.048928	4.562492
239.439775	7165.241203	8.755495	-0.049015	4.564959
239.173733	7173.270329	8.760499	-0.048971	4.567436
239.265006	7181.300388	8.765504	-0.048993	4.569912
239.464657	7189.361828	8.770509	-0.049035	4.572397
239.595683	7197.351929	8.775514	-0.049065	4.574858
239.728602	7205.429562	8.780519	-0.049095	4.577345
240.015445	7213.347808	8.785523	-0.049153	4.579782
240.263136	7221.396409	8.790528	-0.049205	4.582257
240.321134	7229.367642	8.795533	-0.049220	4.584708
240.212922	7237.430972	8.800538	-0.049205	4.587185
240.491433	7245.454081	8.805543	-0.049262	4.589648
240.602212	7253.495165	8.810547	-0.049288	4.592116
240.652736	7261.573310	8.815552	-0.049303	4.594593
240.855714	7269.575132	8.820557	-0.049346	4.597046
240.924699	7277.483638	8.825562	-0.049364	4.599469
241.248534	7285.566376	8.830567	-0.049429	4.601944
241.201909	7293.459047	8.835571	-0.049425	4.604360
241.698499	7301.570872	8.840576	-0.049523	4.606841
241.726036	7309.577201	8.845581	-0.049533	4.609289
241.559395	7317.612400	8.850586	-0.049507	4.611744
241.926714	7325.651745	8.855591	-0.049581	4.614199
242.113954	7333.651520	8.860595	-0.049621	4.616641
242.062982	7341.625865	8.865600	-0.049616	4.619074
242.010410	7349.683266	8.870605	-0.049612	4.621530
242.222931	7357.652880	8.875610	-0.049656	4.623959
242.409924	7365.723132	8.880615	-0.049696	4.626417
242.650780	7373.651114	8.885619	-0.049746	4.628830
242.869922	7381.735214	8.890624	-0.049792	4.631290
243.028951	7389.755841	8.895629	-0.049827	4.633729
242.945993	7397.789622	8.900634	-0.049817	4.636170
243.271576	7405.747134	8.905639	-0.049882	4.638587
243.436403	7413.728153	8.910643	-0.049918	4.641010
243.495207	7421.746113	8.915648	-0.049934	4.643443
243.892851	7429.804126	8.920653	-0.050013	4.645887
243.918641	7437.800680	8.925658	-0.050023	4.648311
243.921675	7445.846716	8.930663	-0.050029	4.650749
244.088072	7453.888186	8.935667	-0.050065	4.653183
244.437056	7461.859193	8.940672	-0.050135	4.655595
244.476412	7469.924286	8.945677	-0.050148	4.658035
244.561361	7477.867775	8.950682	-0.050168	4.660436
244.750074	7485.918103	8.955687	-0.050209	4.662869
244.606612	7493.880413	8.960691	-0.050187	4.665274
244.766523	7501.978391	8.965696	-0.050222	4.667718
244.789402	7509.968301	8.970701	-0.050231	4.670128
245.029178	7518.025473	8.975706	-0.050281	4.672558
245.283976	7526.087011	8.980711	-0.050334	4.674987
245.313998	7534.064659	8.985715	-0.050344	4.677390
245.605470	7542.037392	8.990720	-0.050404	4.679790
245.647854	7550.053490	8.995725	-0.050417	4.682202
245.842291	7557.965557	9.000730	-0.050458	4.684581
246.108130	7566.053548	9.005735	-0.050513	4.687012
245.921335	7574.023651	9.010739	-0.050483	4.689407
246.138827	7582.100056	9.015744	-0.050529	4.691832
246.194212	7590.106881	9.020749	-0.050544	4.694235
246.366896	7598.163360	9.025754	-0.050581	4.696651
246.606878	7606.139104	9.030759	-0.050631	4.699042
246.731161	7614.131763	9.035763	-0.050659	4.701437
247.057651	7622.137277	9.040768	-0.050725	4.703834
247.251916	7630.173173	9.045773	-0.050767	4.706239
247.269699	7638.167069	9.050778	-0.050775	4.708631
247.396012	7646.208686	9.055783	-0.050804	4.711035
247.556449	7654.216079	9.060787	-0.050839	4.713428
247.799676	7662.275315	9.065792	-0.050889	4.715835
247.809587	7670.242725	9.070797	-0.050896	4.718214
248.063924	7678.234012	9.075802	-0.050948	4.720599
248.282145	7686.311842	9.080807	-0.050994	4.723008
248.291778	7694.306158	9.085811	-0.051001	4.725391
248.575219	7702.320610	9.090816	-0.051059	4.727778
248.778291	7710.355268	9.095821	-0.051102	4.730171
248.794592	7718.360853	9.100826	-0.051110	4.732554
248.841097	7726.382321	9.105831	-0.051124	4.734940
248.949770	7734.381167	9.110835	-0.051149	4.737319
248.974818	7742.365387	9.115840	-0.051159	4.739692
249.160283	7750.460375	9.120845	-0.051199	4.742096
249.188012	7758.404365	9.125850	-0.051209	4.744454
249.443965	7766.525200	9.130855	-0.051262	4.746864
249.552011	7774.501286	9.135859	-0.051287	4.749229
249.743547	7782.516018	9.140864	-0.051328	4.751605
249.932466	7790.582236	9.145869	-0.051368	4.753994
249.800065	7798.580415	9.150874	-0.051349	4.756364
250.057633	7806.546949	9.155879	-0.051402	4.758721
250.244390	7814.534652	9.160883	-0.051441	4.761084
250.399441	7822.501737	9.165888	-0.051475	4.763439
250.558041	7830.562677	9.170893	-0.051510	4.765821
250.572438	7838.543495	9.175898	-0.051518	4.768179
250.934273	7846.607708	9.180903	-0.051590	4.770559
250.891815	7854.657204	9.185907	-0.051588	4.772935
250.985255	7862.644703	9.190912	-0.051610	4.775291
251.409005	7870.676526	9.195917	-0.051694	4.777657
251.377690	7878.588831	9.200922	-0.051693	4.779989
251.498531	7886.719085	9.205927	-0.051721	4.782383
251.391755	7894.611691	9.210931	-0.051706	4.784707
251.528641	7902.723729	9.215936	-0.051737	4.787094
251.677291	7910.745543	9.220941	-0.051770	4.789453
251.803746	7918.746626	9.225946	-0.051798	4.791804
252.083951	7926.734787	9.230951	-0.051856	4.794150
252.155335	7934.766450	9.235955	-0.051874	4.796508
252.258488	7942.740867	9.240960	-0.051898	4.798849
252.550141	7950.796567	9.245965	-0.051958	4.801211
252.718497	7958.779929	9.250970	-0.051994	4.803551
252.656321	7966.819105	9.255975	-0.051988	4.805907
252.837260	7974.807378	9.260979	-0.052026	4.808247
252.789873	7982.820537	9.265984	-0.052023	4.810593
252.920652	7990.394437	9.270989	-0.052052	4.812809
253.232488	7994.996745	9.275994	-0.052113	4.814154

253.469328	7997.575121	9.280999	-0.052159	4.814907
253.396981	7998.969199	9.286003	-0.052146	4.815315
253.373740	7999.424673	9.291008	-0.052142	4.815449
253.716483	8000.391100	9.296013	-0.052206	4.815729
253.652967	8000.332404	9.301018	-0.052194	4.815713
253.480532	8000.389383	9.306023	-0.052162	4.815730
253.600731	8000.342213	9.311027	-0.052184	4.815716
253.693667	8000.367202	9.316032	-0.052201	4.815723
253.847428	8000.371825	9.321037	-0.052230	4.815723
253.909990	8000.332260	9.326042	-0.052241	4.815711
254.127937	8000.396649	9.331047	-0.052282	4.815729
254.024565	8000.385351	9.336051	-0.052263	4.815726
253.876763	8000.365857	9.341056	-0.052235	4.815721
254.043716	8000.411267	9.346061	-0.052266	4.815734
254.059625	8000.347455	9.351066	-0.052269	4.815715
253.984842	8000.401750	9.356071	-0.052255	4.815731
253.893045	8000.354339	9.361075	-0.052237	4.815718
254.145811	8000.373383	9.366080	-0.052284	4.815722
254.303255	8000.411165	9.371085	-0.052314	4.815733
254.147698	8000.361650	9.376090	-0.052285	4.815719
254.322046	8000.382623	9.381095	-0.052317	4.815724
254.212757	8000.355213	9.386099	-0.052296	4.815717
254.203824	8000.360397	9.391104	-0.052295	4.815718
254.407786	8000.378649	9.396109	-0.052333	4.815723
254.366740	8000.427086	9.401114	-0.052325	4.815737
254.350974	8000.401196	9.406119	-0.052322	4.815729
254.478044	8000.374423	9.411123	-0.052345	4.815721
254.669199	8000.376452	9.416128	-0.052381	4.815721
254.587522	8000.371912	9.421133	-0.052365	4.815720
254.363165	8000.353309	9.426138	-0.052324	4.815715
254.599929	8000.378500	9.431143	-0.052368	4.815722
254.504591	8000.376942	9.436147	-0.052350	4.815722
254.671163	8000.366826	9.441152	-0.052381	4.815718
254.619260	8000.380921	9.446157	-0.052371	4.815722
254.563592	8000.392819	9.451162	-0.052360	4.815726
254.724782	8000.445611	9.456167	-0.052390	4.815741
254.595467	8000.391182	9.461171	-0.052366	4.815725
254.741859	8000.382875	9.466176	-0.052393	4.815722
254.728039	8000.429619	9.471181	-0.052391	4.815736
254.529434	8000.359117	9.476186	-0.052353	4.815716
254.819557	8000.401191	9.481191	-0.052407	4.815727
254.769746	8000.356597	9.486195	-0.052398	4.815715
254.928832	8000.351698	9.491200	-0.052427	4.815712
254.884078	8000.411820	9.496205	-0.052419	4.815730
254.910372	8000.344973	9.501210	-0.052424	4.815710
254.847152	8000.381305	9.506215	-0.052412	4.815721
254.876849	8000.375372	9.511219	-0.052417	4.815720
254.951439	8000.349882	9.516224	-0.052431	4.815712
255.038039	8000.411071	9.521229	-0.052447	4.815729
255.130290	8000.347431	9.526234	-0.052464	4.815710
255.062070	8000.390088	9.531239	-0.052451	4.815723
255.057673	8000.349434	9.536243	-0.052450	4.815711
255.101310	8000.394978	9.541248	-0.052458	4.815724
255.244465	8000.398363	9.546253	-0.052485	4.815724
255.284438	8000.360565	9.551258	-0.052492	4.815713
254.997568	8000.387924	9.556263	-0.052439	4.815723
255.008729	8000.385960	9.561267	-0.052441	4.815722
254.977229	8000.364084	9.566272	-0.052435	4.815716
255.217796	8000.433115	9.571277	-0.052480	4.815735
255.256545	8000.370740	9.576282	-0.052487	4.815716
255.239136	8000.380057	9.581287	-0.052483	4.815719
255.193621	8000.350479	9.586291	-0.052475	4.815711
255.179718	8000.353447	9.591296	-0.052472	4.815712
255.251214	8000.358870	9.596301	-0.052485	4.815713
255.326740	8000.372901	9.601306	-0.052499	4.815717
255.367903	8000.406659	9.606311	-0.052507	4.815726
255.169781	8000.460018	9.611315	-0.052470	4.815743
255.134797	8000.408189	9.616320	-0.052463	4.815728
255.131183	8000.420933	9.621325	-0.052462	4.815732
255.050867	8000.386519	9.626330	-0.052447	4.815722
255.133141	8000.456180	9.631335	-0.052462	4.815742
255.442773	8000.388599	9.636339	-0.052520	4.815721
255.294784	8000.377642	9.641344	-0.052492	4.815718
255.334088	8000.456215	9.646349	-0.052500	4.815741
255.279299	8000.411538	9.651354	-0.052489	4.815728
255.430635	8000.412921	9.656359	-0.052517	4.815728
255.197704	8000.403786	9.661363	-0.052474	4.815726
255.349759	8000.372081	9.666368	-0.052502	4.815716
255.737009	8000.418940	9.671373	-0.052574	4.815728
255.360126	8000.399991	9.676378	-0.052504	4.815724
255.420600	8000.403100	9.681383	-0.052515	4.815725
255.496306	8000.403253	9.686387	-0.052529	4.815725
255.378379	8000.381040	9.691392	-0.052507	4.815719
255.412717	8000.396536	9.696397	-0.052513	4.815723
255.409667	8000.397545	9.701402	-0.052512	4.815724
255.621155	8000.421260	9.706407	-0.052552	4.815729
255.372896	8000.450313	9.711411	-0.052505	4.815739
255.311850	8000.382045	9.716416	-0.052494	4.815720
255.611213	8000.433882	9.721421	-0.052549	4.815733
255.480412	8000.362344	9.726426	-0.052525	4.815713
255.317768	8000.376774	9.731431	-0.052495	4.815718
255.295179	8000.421241	9.736435	-0.052490	4.815731
255.367371	8000.444827	9.741440	-0.052504	4.815738
255.341919	8000.416643	9.746445	-0.052499	4.815729
255.271573	8000.355698	9.751450	-0.052485	4.815712
255.459881	8000.385442	9.756455	-0.052520	4.815720
255.390748	8000.397121	9.761459	-0.052507	4.815724
255.560092	8000.358223	9.766464	-0.052539	4.815711
255.662047	8000.403648	9.771469	-0.052558	4.815724
255.264679	8000.406787	9.776474	-0.052484	4.815727
255.517172	8000.421560	9.781479	-0.052531	4.815730
255.553310	8000.476591	9.786483	-0.052537	4.815746
255.546746	8000.411344	9.791488	-0.052536	4.815727
255.532128	8000.408961	9.796493	-0.052533	4.815726
255.534782	8000.367354	9.801498	-0.052533	4.815714
255.680078	8000.410279	9.806503	-0.052560	4.815726
255.472169	8000.460275	9.811507	-0.052522	4.815742
255.420075	8000.386814	9.816512	-0.052512	4.815720
255.695603	8000.377403	9.821517	-0.052563	4.815716
255.562950	8000.348544	9.826522	-0.052538	4.815709
255.603571	8000.425003	9.831527	-0.052546	4.815731
255.772578	8000.414928	9.836531	-0.052577	4.815727
255.508866	8000.382871	9.841536	-0.052528	4.815719
255.495365	8000.450975	9.846541	-0.052525	4.815739
255.492053	8000.347343	9.851546	-0.052524	4.815709
255.726294	8000.367157	9.856551	-0.052568	4.815713
255.730123	8000.386429	9.861555	-0.052568	4.815719
255.759183	8000.367673	9.866560	-0.052574	4.815713
255.882111	8000.431590	9.871565	-0.052597	4.815731
255.733905	8000.400342	9.876570	-0.052569	4.815723
255.622288	8000.424143	9.881575	-0.052548	4.815730
255.585437	8000.479055	9.886579	-0.052541	4.815747
255.688911	8000.397446	9.891584	-0.052560	4.815722
255.699724	8000.434982	9.896589	-0.052562	4.815733
255.743125	8000.420730	9.901594	-0.052570	4.815729
255.856258	8000.416153	9.906599	-0.052591	4.815727
255.813502	8000.429329	9.911603	-0.052583	4.815731
255.705466	8000.365635	9.916608	-0.052563	4.815713
255.774080	8000.415856	9.921613	-0.052575	4.815727
255.907599	8000.395595	9.926618	-0.052600	4.815721
255.801895	8000.399205	9.931623	-0.052580	4.815722
256.007814	8000.509317	9.936627	-0.052619	4.815754
256.142863	8000.426084	9.941632	-0.052644	4.815729
255.903095	8000.528949	9.946637	-0.052599	4.815760
255.834920	8000.439209	9.951642	-0.052586	4.815734
255.932796	8000.430114	9.956647	-0.052604	4.815731
255.891581	8000.421960	9.961651	-0.052596	4.815729
255.685854	8000.372693	9.966656	-0.052558	4.815715
255.760849	8000.411273	9.971661	-0.052572	4.815726
255.804100	8000.372461	9.976666	-0.052580	4.815715
255.739761	8000.361796	9.981671	-0.052568	4.815712
255.710885	8000.383738	9.986675	-0.052562	4.815718
256.020147	8000.384486	9.991680	-0.052620	4.815717
255.883875	8000.438850	9.996685	-0.052594	4.815734
255.901169	8000.383600	10.001690	-0.052597	4.815717
256.032517	8000.414555	10.006695	-0.052622	4.815726
255.950189	8000.431358	10.011699	-0.052606	4.815731
255.933939	8000.363817	10.016704	-0.052603	4.815711
256.109605	8000.427524	10.021709	-0.052636	4.815729
255.994373	8000.383999	10.026714	-0.052614	4.815717
256.020039	8000.429251	10.031719	-0.052619	4.815730
256.075603	8000.368217	10.036723	-0.052629	4.815712
255.868775	8000.378725	10.041728	-0.052590	4.815716
255.920477	8000.440416	10.046733	-0.052600	4.815734
255.792547	8000.416972	10.051738	-0.052576	4.815728
255.894068	8000.421816	10.056743	-0.052595	4.815729
255.933536	8000.423516	10.061747	-0.052602	4.815729
255.641120	8000.388856	10.066752	-0.052547	4.815720
255.865055	8000.374335	10.071757	-0.052589	4.815715
255.819143	8000.360767	10.076762	-0.052580	4.815711
255.944507	8000.394827	10.081767	-0.052604	4.815720
255.872474	8000.374427	10.086771	-0.052590	4.815715
256.150606	8000.354382	10.091776	-0.052642	4.815708
255.982284	8000.381532	10.096781	-0.052610	4.815716
255.983849	8000.374073	10.101786	-0.052610	4.815714
255.922051	8000.400820	10.106791	-0.052599	4.815722
256.080352	8000.403384	10.111795	-0.052628	4.815722
256.110587	8000.400663	10.116800	-0.052634	4.815721
255.915224	8000.489301	10.121805	-0.052597	4.815748
256.041388	8000.414466	10.126810	-0.052621	4.815726
255.831166	8000.421716	10.131815	-0.052581	4.815729
255.784416	8000.400659	10.136819	-0.052572	4.815723
255.933814	8000.364641	10.141824	-0.052600	4.815712
255.882240	8000.396892	10.146829	-0.052590	4.815721
255.711194	8000.349257	10.151834	-0.052558	4.815708
255.875250	8000.428791	10.156839	-0.052589	4.815731
255.879005	8000.446993	10.161843	-0.052590	4.815736
255.849511	8000.368560	10.166848	-0.052584	4.815713
255.744110	8000.390327	10.171853	-0.052564	4.815720
255.849276	8000.401636	10.176858	-0.052584	4.815723
255.885773	8000.376595	10.181863	-0.052590	4.815715
255.860351	8000.407136	10.186867	-0.052586	4.815724
255.822052	8000.374472	10.191872	-0.052578	4.815715
256.051537	8000.435850	10.196877	-0.052621	4.815732
255.959538	8000.468512	10.201882	-0.052604	4.815742
256.173062	8000.471975	10.206887	-0.052643	4.815742
255.973345	8000.427076	10.211891	-0.052606	4.815730
255.874953	8000.354997	10.216896	-0.052588	4.815709
255.909002	8000.430281	10.221901	-0.052594	4.815731
255.792135	8000.374985	10.226906	-0.052572	4.815715
255.983930	8000.403719	10.231911	-0.052608	4.815723
256.001471	8000.427485	10.236915	-0.052611	4.815730
255.969822	8000.388522	10.241920	-0.052605	4.815719
256.202948	8000.420064	10.246925	-0.052648	4.815727
256.005125	8000.380535	10.251930	-0.052611	4.815716
256.049923	8000.423963	10.256935	-0.052619	4.815729
256.110269	8000.440951	10.261939	-0.052630	4.815733
256.057760	8000.433681	10.266944	-0.052621	4.815731
256.193161	8000.451889	10.271949	-0.052646	4.815736
256.102277	8000.427979	10.276954	-0.052629	4.815729
256.063641	8000.401715	10.281959	-0.052621	4.815722
256.026195	8000.387216	10.286963	-0.052614	4.815718
256.018011	8000.388141	10.291968	-0.052613	4.815718
256.172651	8000.418407	10.296973	-0.052641	4.815726
256.031354	8000.419303	10.301978	-0.052615	4.815727
255.963904	8000.361607	10.306983	-0.052602	4.815711
256.154730	8000.390326	10.311987	-0.052638	4.815718
255.879170	8000.375158	10.316992	-0.052586	4.815715
256.033403	8000.484429	10.321997	-0.052615	4.815746
256.136054	8000.413483	10.327002	-0.052634	4.815725
256.007573	8000.382555	10.332007	-0.052610	4.815717
256.089585	8000.392421	10.337011	-0.052625	4.815719
256.008297	8000.396428	10.342016	-0.052610	4.815721
256.036627	8000.413963	10.347021	-0.052615	4.815726
256.047402	8000.409857	10.352026	-0.052617	4.815724
256.170019	8000.375539	10.357031	-0.052639	4.815714
256.307205	8000.400182	10.362035	-0.052665	4.815720
255.915817	8000.356438	10.367040	-0.052592	4.815710
255.960240	8000.431892	10.372045	-0.052600	4.815731
255.886560	8000.425345	10.377050	-0.052586	4.815730
255.944396	8000.433750	10.382055	-0.052597	4.815732
256.004863	8000.461417	10.387059	-0.052608	4.815740
255.808779	8000.418713	10.392064	-0.052571	4.815728
256.196953	8000.411134	10.397069	-0.052644	4.815724
256.103854	8000.406408	10.402074	-0.052626	4.815723
256.071116	8000.394121	10.407079	-0.052620	4.815720
256.075016	8000.370684	10.412083	-0.052620	4.815713
256.102104	8000.376454	10.417088	-0.052625	4.815715
256.206941	8000.384555	10.422093	-0.052645	4.815716
256.204048	8000.363144	10.427098	-0.052644	4.815710
256.260814	8000.370463	10.432103	-0.052655	4.815712
256.221740	8000.424273	10.437107	-0.052647	4.815728
256.107264	8000.374354	10.442112	-0.052626	4.815714
256.262140	8000.441994	10.447117	-0.052655	4.815733
256.191495	8000.429091	10.452122	-0.052641	4.815729
256.011037	8000.405860	10.457127	-0.052608	4.815724
256.088457	8000.410312	10.462131	-0.052622	4.815724
256.151329	8000.401715	10.467136	-0.052633	4.815722
256.204532	8000.461296	10.472141	-0.052643	4.815739
256.148019	8000.415522	10.477146	-0.052633	4.815726
256.234940	8000.422265	10.482151	-0.052649	4.815727
256.295755	8000.417905	10.487155	-0.052660	4.815726
256.122377	8000.362758	10.492160	-0.052628	4.815710
256.178828	8000.422391	10.497165	-0.052638	4.815728
256.265450	8000.357591	10.502170	-0.052654	4.815708
256.250455	8000.380827	10.507175	-0.052651	4.815715
256.443710	8000.434144	10.512179	-0.052687	4.815730
256.453541	8000.355281	10.517184	-0.052689	4.815707
256.482692	8000.423013	10.522189	-0.052694	4.815726
256.169883	8000.458490	10.527194	-0.052636	4.815738
256.190122	8000.407559	10.532199	-0.052639	4.815723
256.236297	8000.386945	10.537203	-0.052648	4.815717
256.205291	8000.358670	10.542208	-0.052642	4.815709
256.095437	8000.387839	10.547213	-0.052621	4.815718
256.147038	8000.351297	10.552218	-0.052631	4.815707
256.251583	8000.390358	10.557223	-0.052650	4.815718
256.313037	8000.420177	10.562227	-0.052661	4.815726
256.313790	8000.360386	10.567232	-0.052661	4.815709
256.280075	8000.417486	10.572237	-0.052655	4.815726
256.201818	8000.393781	10.577242	-0.052640	4.815719
256.298309	8000.398544	10.582247	-0.052658	4.815720
256.456764	8000.469446	10.587251	-0.052688	4.815740
256.149187	8000.402506	10.592256	-0.052630	4.815722
256.312869	8000.416903	10.597261	-0.052661	4.815725
256.383859	8000.446877	10.602266	-0.052674	4.815734
256.275105	8000.408795	10.607271	-0.052653	4.815723
256.142258	8000.435454	10.612275	-0.052629	4.815732
256.146296	8000.387462	10.617280	-0.052629	4.815718
256.317377	8000.398776	10.622285	-0.052661	4.815720
256.116837	8000.394438	10.627290	-0.052624	4.815720
256.088074	8000.399299	10.632295	-0.052618	4.815721
256.119735	8000.400872	10.637299	-0.052624	4.815722
256.102726	8000.370689	10.642304	-0.052621	4.815713
256.409177	8000.410898	10.647309	-0.052678	4.815723
256.227622	8000.401530	10.652314	-0.052644	4.815721
256.059929	8000.368897	10.657319	-0.052612	4.815713
256.139684	8000.417164	10.662323	-0.052627	4.815726
256.332782	8000.358366	10.667328	-0.052663	4.815708
256.344376	8000.389509	10.672333	-0.052665	4.815717
256.140621	8000.360561	10.677338	-0.052627	4.815710
256.269926	8000.354111	10.682343	-0.052651	4.815707
256.450827	8000.374127	10.687347	-0.052684	4.815712
256.210782	8000.406517	10.692352	-0.052640	4.815723
256.312172	8000.411359	10.697357	-0.052658	4.815724
256.352167	8000.404526	10.702362	-0.052666	4.815722
256.442704	8000.426275	10.707367	-0.052682	4.815728
256.360110	8000.429193	10.712371	-0.052667	4.815729
256.423121	8000.403515	10.717376	-0.052679	4.815721
256.379283	8000.403860	10.722381	-0.052670	4.815721
256.213869	8000.378738	10.727386	-0.052639	4.815715
256.109749	8000.394119	10.732391	-0.052620	4.815720
256.227658	8000.447278	10.737395	-0.052642	4.815735
256.265598	8000.353925	10.742400	-0.052649	4.815707
256.197510	8000.396585	10.747405	-0.052636	4.815720
256.232165	8000.373649	10.752410	-0.052642	4.815713
256.324827	8000.379417	10.757415	-0.052659	4.815715
256.266203	8000.405147	10.762419	-0.052648	4.815722
256.253692	8000.377173	10.767424	-0.052646	4.815714
256.421675	8000.435417	10.772429	-0.052677	4.815730
256.236535	8000.432397	10.777434	-0.052642	4.815730
256.172327	8000.451630	10.782439	-0.052630	4.815736
256.451002	8000.500997	10.787443	-0.052682	4.815749
256.361862	8000.435473	10.792448	-0.052665	4.815731
256.455045	8000.419895	10.797453	-0.052683	4.815726
256.398119	8000.409350	10.802458	-0.052672	4.815723
256.176431	8000.391855	10.807463	-0.052631	4.815719
256.151593	8000.427744	10.812467	-0.052626	4.815729
256.245206	8000.379074	10.817472	-0.052643	4.815715
256.571702	8000.426015	10.822477	-0.052704	4.815727
256.448828	8000.447497	10.827482	-0.052681	4.815734
256.353659	8000.390418	10.832487	-0.052663	4.815718
256.646555	8000.433610	10.837491	-0.052718	4.815729
256.240216	8000.394960	10.842496	-0.052642	4.815720
256.352006	8000.407445	10.847501	-0.052662	4.815723
256.424957	8000.386200	10.852506	-0.052676	4.815716
256.451668	8000.410115	10.857511	-0.052681	4.815723
256.411153	8000.471375	10.862515	-0.052673	4.815741
256.343779	8000.452118	10.867520	-0.052660	4.815736
256.500714	8000.463202	10.872525	-0.052690	4.815738
256.286001	8000.436211	10.877530	-0.052649	4.815731
256.418243	8000.436216	10.882535	-0.052674	4.815731
256.506628	8000.481421	10.887539	-0.052690	4.815744
256.371936	8000.421563	10.892544	-0.052665	4.815727
256.373878	8000.403433	10.897549	-0.052665	4.815721
256.553836	8000.415960	10.902554	-0.052699	4.815724
256.588259	8000.399426	10.907559	-0.052705	4.815719
256.374325	8000.404479	10.912563	-0.052665	4.815722
256.366317	8000.332801	10.917568	-0.052663	4.815701
256.633316	8000.469533	10.922573	-0.052713	4.815739
256.599201	8000.454020	10.927578	-0.052707	4.815735
256.301317	8000.402186	10.932583	-0.052651	4.815721
256.392670	8000.445303	10.937587	-0.052668	4.815734
256.505271	8000.405483	10.942592	-0.052689	4.815721
256.424133	8000.456473	10.947597	-0.052674	4.815737
256.339578	8000.450817	10.952602	-0.052658	4.815735
256.379071	8000.385250	10.957607	-0.052665	4.815716
256.353698	8000.409386	10.962611	-0.052660	4.815723
256.269296	8000.382378	10.967616	-0.052644	4.815716
256.476638	8000.490378	10.972621	-0.052683	4.815746
256.440622	8000.486580	10.977626	-0.052676	4.815745
256.467354	8000.459244	10.982631	-0.052681	4.815737
256.553819	8000.536450	10.987635	-0.052697	4.815759
256.466996	8000.482709	10.992640	-0.052681	4.815744
256.337281	8000.430406	10.997645	-0.052656	4.815729
256.703221	8000.390434	11.002650	-0.052724	4.815716
256.686452	8000.448878	11.007655	-0.052721	4.815733
256.792247	8000.519993	11.012659	-0.052741	4.815754
256.669372	8000.436836	11.017664	-0.052718	4.815730
256.723076	8000.428090	11.022669	-0.052728	4.815727
256.516279	8000.430055	11.027674	-0.052689	4.815729
256.547738	8000.429490	11.032679	-0.052695	4.815728
256.625510	8000.460642	11.037683	-0.052709	4.815737
256.720698	8000.440825	11.042688	-0.052727	4.815731
256.695090	8000.457483	11.047693	-0.052722	4.815736
256.561026	8000.405109	11.052698	-0.052697	4.815721
256.662509	8000.383259	11.057703	-0.052716	4.815714
256.539509	8000.530733	11.062707	-0.052693	4.815758
256.443857	8000.461900	11.067712	-0.052675	4.815738
256.519693	8000.417211	11.072717	-0.052689	4.815725
256.782508	8000.409730	11.077722	-0.052737	4.815721
256.518485	8000.421443	11.082727	-0.052688	4.815726
256.507202	8000.424453	11.087731	-0.052686	4.815727
256.530342	8000.405600	11.092736	-0.052690	4.815721
256.430941	8000.434938	11.097741	-0.052672	4.815730
256.627317	8000.509661	11.102746	-0.052708	4.815751
256.708909	8000.422356	11.107751	-0.052723	4.815725
256.696350	8000.468055	11.112755	-0.052721	4.815739
256.446058	8000.419129	11.117760	-0.052674	4.815726
256.545517	8000.451702	11.122765	-0.052692	4.815735
256.589513	8000.454543	11.127770	-0.052700	4.815735
256.609371	8000.415350	11.132775	-0.052704	4.815724
256.494985	8000.422022	11.137779	-0.052683	4.815726
256.578265	8000.413757	11.142784	-0.052698	4.815724
256.504765	8000.430703	11.147789	-0.052684	4.815729
256.546291	8000.435640	11.152794	-0.052692	4.815730
256.696235	8000.400698	11.157799	-0.052720	4.815719
256.710943	8000.500228	11.162803	-0.052722	4.815748
256.587452	8000.458703	11.167808	-0.052699	4.815737
256.686888	8000.445362	11.172813	-0.052718	4.815732
256.595192	8000.458809	11.177818	-0.052700	4.815737
256.466210	8000.406518	11.182823	-0.052676	4.815722
256.406875	8000.470676	11.187827	-0.052665	4.815741
256.572013	8000.443455	11.192832	-0.052696	4.815732
256.616934	8000.466599	11.197837	-0.052704	4.815739
256.645912	8000.508702	11.202842	-0.052709	4.815751
256.653127	8000.413781	11.207847	-0.052711	4.815723
256.604731	8000.429000	11.212851	-0.052701	4.815728
256.557667	8000.385515	11.217856	-0.052692	4.815715
256.635004	8000.398508	11.222861	-0.052707	4.815719
256.713565	8000.346389	11.227866	-0.052721	4.815703
256.618745	8000.384344	11.232871	-0.052704	4.815715
256.586351	8000.468159	11.237875	-0.052697	4.815739
256.522648	8000.417997	11.242880	-0.052685	4.815725
256.531470	8000.425605	11.247885	-0.052687	4.815727
256.426758	8000.475144	11.252890	-0.052667	4.815742
256.393181	8000.417998	11.257895	-0.052661	4.815726
256.701687	8000.447564	11.262899	-0.052718	4.815733
256.328237	8000.421194	11.267904	-0.052649	4.815727
256.467537	8000.433059	11.272909	-0.052675	4.815730
256.499228	8000.463461	11.277914	-0.052680	4.815739
256.521492	8000.380530	11.282919	-0.052684	4.815714
256.459818	8000.469208	11.287923	-0.052673	4.815740
256.403409	8000.438384	11.292928	-0.052662	4.815732
256.508908	8000.451835	11.297933	-0.052682	4.815735
256.597963	8000.477832	11.302938	-0.052698	4.815742
256.552838	8000.441853	11.307943	-0.052690	4.815732
256.614011	8000.424686	11.312947	-0.052701	4.815727
256.601635	8000.365750	11.317952	-0.052698	4.815710
256.613421	8000.379812	11.322957	-0.052701	4.815714
256.784880	8000.470146	11.327962	-0.052732	4.815739
256.605892	8000.401025	11.332967	-0.052699	4.815720
256.508571	8000.404771	11.337971	-0.052681	4.815721
256.628785	8000.345856	11.342976	-0.052703	4.815704
256.780376	8000.409173	11.347981	-0.052731	4.815721
256.747679	8000.452409	11.352986	-0.052725	4.815734
256.789527	8000.432792	11.357991	-0.052733	4.815728
256.718381	8000.450845	11.362995	-0.052719	4.815734
256.815515	8000.369131	11.368000	-0.052737	4.815710
256.577585	8000.403691	11.373005	-0.052693	4.815721
256.689252	8000.443936	11.378010	-0.052713	4.815732
256.605568	8000.421210	11.383015	-0.052698	4.815726
256.502892	8000.435547	11.388019	-0.052679	4.815730
256.604278	8000.396612	11.393024	-0.052697	4.815719
256.514622	8000.411160	11.398029	-0.052681	4.815723
256.689104	8000.386227	11.403034	-0.052713	4.815715
256.718078	8000.369604	11.408039	-0.052718	4.815710
256.855302	8000.391046	11.413043	-0.052744	4.815716
256.731758	8000.409314	11.418048	-0.052720	4.815722
256.861620	8000.423162	11.423053	-0.052745	4.815725
256.841464	8000.379047	11.428058	-0.052741	4.815712
256.925747	8000.428456	11.433063	-0.052756	4.815726
256.688086	8000.445936	11.438067	-0.052712	4.815733
256.785326	8000.424017	11.443072	-0.052730	4.815726
256.710298	8000.390755	11.448077	-0.052716	4.815716
256.740968	8000.421141	11.453082	-0.052721	4.815725
256.509879	8000.387477	11.458087	-0.052678	4.815716
256.644872	8000.432372	11.463091	-0.052703	4.815729
256.659000	8000.398424	11.468096	-0.052706	4.815719
256.768473	8000.429024	11.473101	-0.052726	4.815727
256.693674	8000.382953	11.478106	-0.052712	4.815714
256.573139	8000.379915	11.483111	-0.052689	4.815714
256.665465	8000.481774	11.488115	-0.052707	4.815743
256.786285	8000.459172	11.493120	-0.052729	4.815736
257.056839	8000.418717	11.498125	-0.052779	4.815723
256.831401	8000.484444	11.503130	-0.052737	4.815743
256.688681	8000.405236	11.508135	-0.052710	4.815721
256.814640	8000.486288	11.513139	-0.052734	4.815744
256.623744	8000.503460	11.518144	-0.052698	4.815750
256.688993	8000.422296	11.523149	-0.052710	4.815726
256.608064	8000.435918	11.528154	-0.052695	4.815730
256.842201	8000.366042	11.533159	-0.052738	4.815709
256.939702	8000.441293	11.538163	-0.052757	4.815730
256.734922	8000.428343	11.543168	-0.052718	4.815727
256.766067	8000.472617	11.548173	-0.052724	4.815740
256.973718	8000.409785	11.553178	-0.052763	4.815721
256.636989	8000.423518	11.558183	-0.052700	4.815726
256.705790	8000.457727	11.563187	-0.052712	4.815736
256.687299	8000.484110	11.568192	-0.052709	4.815744
256.669287	8000.433624	11.573197	-0.052705	4.815729
256.800785	8000.481666	11.578202	-0.052730	4.815743
256.964702	8000.406377	11.583207	-0.052760	4.815720
256.878497	8000.438065	11.588211	-0.052744	4.815729
256.746955	8000.435916	11.593216	-0.052719	4.815729
257.076033	8000.411362	11.598221	-0.052781	4.815721
257.031877	8000.442666	11.603226	-0.052772	4.815730
256.790305	8000.417372	11.608231	-0.052727	4.815724
256.937914	8000.443254	11.613235	-0.052755	4.815731
256.986551	8000.467526	11.618240	-0.052764	4.815738
256.876221	8000.430486	11.623245	-0.052743	4.815727
256.650817	8000.456707	11.628250	-0.052701	4.815736
256.795337	8000.414203	11.633255	-0.052728	4.815723
256.874467	8000.438970	11.638259	-0.052742	4.815730
256.622945	8000.427395	11.643264	-0.052695	4.815728
256.791387	8000.406635	11.648269	-0.052726	4.815721
256.727146	8000.457900	11.653274	-0.052714	4.815736
256.542095	8000.436729	11.658279	-0.052680	4.815731
256.820561	8000.456197	11.663283	-0.052732	4.815735
256.676052	8000.416466	11.668288	-0.052705	4.815724
256.669058	8000.421681	11.673293	-0.052703	4.815726
256.712964	8000.420250	11.678298	-0.052711	4.815725
256.773285	8000.399866	11.683303	-0.052722	4.815719
256.747268	8000.420788	11.688307	-0.052717	4.815725
256.785804	8000.374425	11.693312	-0.052724	4.815711
256.941339	8000.358793	11.698317	-0.052753	4.815706
257.137068	8000.438845	11.703322	-0.052790	4.815729
256.936067	8000.401398	11.708327	-0.052752	4.815719
256.834974	8000.509722	11.713331	-0.052733	4.815751
256.890849	8000.479656	11.718336	-0.052744	4.815742
256.754266	8000.398412	11.723341	-0.052718	4.815719
256.840365	8000.445715	11.728346	-0.052734	4.815732
256.979526	8000.392446	11.733351	-0.052760	4.815716
256.871330	8000.412032	11.738355	-0.052739	4.815722
256.884672	8000.415442	11.743360	-0.052742	4.815723
256.925091	8000.415022	11.748365	-0.052749	4.815723
257.075223	8000.558398	11.753370	-0.052777	4.815764
256.972273	8000.568459	11.758375	-0.052758	4.815767
256.886131	8000.559574	11.763379	-0.052742	4.815765
256.669611	8000.569923	11.768384	-0.052701	4.815769
256.624541	8000.443186	11.773389	-0.052693	4.815732
256.694749	8000.501976	11.778394	-0.052706	4.815749
256.704364	8000.432719	11.783399	-0.052707	4.815729
256.878472	8000.417390	11.788403	-0.052740	4.815724
256.791574	8000.422373	11.793408	-0.052723	4.815725
256.842823	8000.426400	11.798413	-0.052733	4.815726
256.820084	8000.371566	11.803418	-0.052728	4.815710
256.530745	8000.423441	11.808423	-0.052674	4.815727
256.606646	8000.510085	11.813427	-0.052689	4.815752
256.738813	8000.494073	11.818432	-0.052713	4.815747
256.697725	8000.427195	11.823437	-0.052705	4.815727
256.793187	8000.426603	11.828442	-0.052723	4.815727
256.655631	8000.398730	11.833447	-0.052697	4.815719
256.940242	8000.443924	11.838451	-0.052750	4.815731
256.813727	8000.472821	11.843456	-0.052726	4.815740
256.608640	8000.442782	11.848461	-0.052688	4.815732
256.915465	8000.488337	11.853466	-0.052745	4.815744
256.714854	8000.437016	11.858471	-0.052708	4.815730
256.682528	8000.426871	11.863475	-0.052701	4.815727
256.856950	8000.404072	11.868480	-0.052734	4.815720
256.903615	8000.408024	11.873485	-0.052742	4.815721
256.942282	8000.481251	11.878490	-0.052750	4.815742
256.882939	8000.398059	11.883495	-0.052738	4.815718
257.031143	8000.448509	11.888499	-0.052766	4.815732
257.023415	8000.446238	11.893504	-0.052764	4.815731
256.846478	8000.419860	11.898509	-0.052731	4.815724
256.948059	8000.467415	11.903514	-0.052750	4.815738
256.877107	8000.422474	11.908519	-0.052737	4.815725
256.742490	8000.453375	11.913523	-0.052712	4.815735
256.916127	8000.445512	11.918528	-0.052744	4.815732
256.847514	8000.413422	11.923533	-0.052731	4.815723
256.891937	8000.421609	11.928538	-0.052739	4.815725
256.720838	8000.426290	11.933543	-0.052707	4.815727
256.889153	8000.426883	11.938547	-0.052738	4.815726
257.031478	8000.435594	11.943552	-0.052765	4.815728
256.754368	8000.466313	11.948557	-0.052713	4.815739
256.667882	8000.488387	11.953562	-0.052697	4.815745
256.672189	8000.400893	11.958567	-0.052697	4.815720
256.668459	8000.446735	11.963571	-0.052697	4.815733
256.731751	8000.430671	11.968576	-0.052708	4.815728
256.643382	8000.414276	11.973581	-0.052692	4.815724
256.716300	8000.469907	11.978586	-0.052705	4.815740
256.722520	8000.389918	11.983591	-0.052706	4.815716
256.826436	8000.451392	11.988595	-0.052726	4.815734
256.872266	8000.476686	11.993600	-0.052734	4.815741
256.737809	8000.439253	11.998605	-0.052709	4.815731
256.742612	8000.479896	12.003610	-0.052710	4.815743
256.924654	8000.428392	12.008615	-0.052743	4.815727
256.749970	8000.454370	12.013619	-0.052711	4.815735
256.714912	8000.446316	12.018624	-0.052704	4.815733
256.829007	8000.413995	12.023629	-0.052725	4.815723
256.764889	8000.452449	12.028634	-0.052713	4.815734
256.763961	8000.416121	12.033639	-0.052713	4.815724
256.830910	8000.448164	12.038643	-0.052725	4.815733
256.799436	8000.433762	12.043648	-0.052719	4.815729
256.743346	8000.401876	12.048653	-0.052709	4.815720
256.729574	8000.434742	12.053658	-0.052706	4.815729
256.613231	8000.484092	12.058663	-0.052684	4.815744
256.836391	8000.473831	12.063667	-0.052726	4.815740
256.765391	8000.457718	12.068672	-0.052712	4.815736
256.708304	8000.455712	12.073677	-0.052702	4.815736
256.831681	8000.473725	12.078682	-0.052725	4.815740
256.636107	8000.405402	12.083687	-0.052688	4.815721
256.847037	8000.446194	12.088691	-0.052727	4.815732
256.892976	8000.448000	12.093696	-0.052736	4.815733
256.817338	8000.416863	12.098701	-0.052721	4.815724
256.902325	8000.459877	12.103706	-0.052737	4.815736
256.778515	8000.382044	12.108711	-0.052714	4.815714
256.938545	8000.422008	12.113715	-0.052744	4.815725
256.899546	8000.469413	12.118720	-0.052736	4.815739
256.946480	8000.508606	12.123725	-0.052745	4.815750
256.741240	8000.484970	12.128730	-0.052707	4.815744
256.528233	8000.397145	12.133735	-0.052667	4.815720
256.914885	8000.487775	12.138739	-0.052739	4.815744
256.897741	8000.473606	12.143744	-0.052735	4.815740
256.771285	8000.380781	12.148749	-0.052712	4.815714
256.814544	8000.399627	12.153754	-0.052720	4.815719
256.797464	8000.382256	12.158759	-0.052716	4.815714
256.867482	8000.405807	12.163763	-0.052729	4.815720
256.674146	8000.409060	12.168768	-0.052693	4.815722
256.901853	8000.379653	12.173773	-0.052735	4.815713
256.936557	8000.425053	12.178778	-0.052742	4.815726
256.832500	8000.384912	12.183783	-0.052722	4.815715
257.113132	8000.421500	12.188787	-0.052774	4.815724
256.986632	8000.446126	12.193792	-0.052751	4.815732
256.841247	8000.387161	12.198797	-0.052724	4.815715
256.858901	8000.446164	12.203802	-0.052727	4.815732
257.000574	8000.394004	12.208807	-0.052753	4.815716
256.960074	8000.406149	12.213811	-0.052745	4.815720
256.725837	8000.410871	12.218816	-0.052702	4.815723
256.863918	8000.426988	12.223821	-0.052727	4.815727
256.776136	8000.437296	12.228826	-0.052711	4.815730
256.736183	8000.398197	12.233831	-0.052703	4.815719
256.942072	8000.382317	12.238835	-0.052741	4.815713
256.870809	8000.373674	12.243840	-0.052728	4.815711
256.839269	8000.371016	12.248845	-0.052722	4.815710
256.823368	8000.443354	12.253850	-0.052719	4.815732
257.121316	8000.353161	12.258855	-0.052774	4.815704
257.044291	8000.419167	12.263859	-0.052760	4.815724
257.012092	8000.425040	12.268864	-0.052754	4.815725
256.968216	8000.406165	12.273869	-0.052746	4.815720
257.182799	8000.451288	12.278874	-0.052785	4.815732
257.062709	8000.388463	12.283879	-0.052763	4.815715
256.990399	8000.424648	12.288883	-0.052749	4.815725
256.952856	8000.445383	12.293888	-0.052742	4.815732
256.945663	8000.424969	12.298893	-0.052741	4.815726
256.916436	8000.450110	12.303898	-0.052735	4.815733
257.161403	8000.437001	12.308903	-0.052781	4.815728
257.296837	8000.430652	12.313907	-0.052806	4.815726
257.004672	8000.481413	12.318912	-0.052751	4.815742
256.999568	8000.463168	12.323917	-0.052750	4.815737
257.172850	8000.504417	12.328922	-0.052783	4.815748
256.910309	8000.422191	12.333927	-0.052733	4.815725
256.963657	8000.440133	12.338931	-0.052743	4.815730
256.992740	8000.429918	12.343936	-0.052749	4.815727
256.882796	8000.365124	12.348941	-0.052728	4.815709
256.835343	8000.395307	12.353946	-0.052719	4.815718
256.768938	8000.405962	12.358951	-0.052707	4.815721
256.936284	8000.466333	12.363955	-0.052738	4.815738
256.801873	8000.475882	12.368960	-0.052713	4.815741
256.868510	8000.417162	12.373965	-0.052725	4.815724
257.128750	8000.449147	12.378970	-0.052773	4.815732
257.015314	8000.423802	12.383975	-0.052752	4.815725
256.909461	8000.447696	12.388979	-0.052732	4.815733
257.041003	8000.423132	12.393984	-0.052756	4.815725
257.102128	8000.389949	12.398989	-0.052768	4.815715
257.187531	8000.471410	12.403994	-0.052784	4.815738
257.134075	8000.427820	12.408999	-0.052773	4.815726
257.115517	8000.428577	12.414003	-0.052770	4.815726
256.969099	8000.425118	12.419008	-0.052743	4.815726
257.002852	8000.382947	12.424013	-0.052749	4.815713
257.023380	8000.451607	12.429018	-0.052752	4.815733
256.843139	8000.381398	12.434023	-0.052719	4.815714
256.798837	8000.394548	12.439027	-0.052710	4.815718
256.975700	8000.415567	12.444032	-0.052743	4.815723
256.987608	8000.401870	12.449037	-0.052745	4.815719
257.067457	8000.475766	12.454042	-0.052760	4.815740
256.805003	8000.451200	12.459047	-0.052711	4.815734
257.151909	8000.422665	12.464051	-0.052776	4.815724
256.995395	8000.437194	12.469056	-0.052746	4.815729
256.978457	8000.394199	12.474061	-0.052743	4.815717
256.882578	8000.465236	12.479066	-0.052725	4.815738
256.909609	8000.397330	12.484071	-0.052730	4.815718
257.018922	8000.436470	12.489075	-0.052750	4.815729
257.135506	8000.456508	12.494080	-0.052772	4.815734
257.050523	8000.400661	12.499085	-0.052756	4.815718
257.028770	8000.438736	12.504090	-0.052752	4.815729
257.024406	8000.403420	12.509095	-0.052751	4.815719
257.134411	8000.394522	12.514099	-0.052771	4.815716
256.969626	8000.466575	12.519104	-0.052740	4.815738
256.859974	8000.393243	12.524109	-0.052720	4.815717
256.971517	8000.446299	12.529114	-0.052741	4.815732
256.962427	8000.421583	12.534119	-0.052739	4.815725
257.044708	8000.414370	12.539123	-0.052754	4.815722
256.975534	8000.452742	12.544128	-0.052741	4.815734
256.809147	8000.413722	12.549133	-0.052710	4.815723
256.802610	8000.475535	12.554138	-0.052709	4.815741
256.788734	8000.463555	12.559143	-0.052706	4.815738
257.167514	8000.400303	12.564147	-0.052776	4.815718
257.067312	8000.418950	12.569152	-0.052757	4.815724
257.041276	8000.437737	12.574157	-0.052753	4.815729
257.127427	8000.372928	12.579162	-0.052768	4.815710
257.005773	8000.457427	12.584167	-0.052746	4.815735
257.142491	8000.428676	12.589171	-0.052771	4.815726
256.914306	8000.463394	12.594176	-0.052728	4.815737
256.811963	8000.405129	12.599181	-0.052709	4.815721
256.869009	8000.429538	12.604186	-0.052720	4.815728
256.874106	8000.355937	12.609191	-0.052721	4.815706
257.088031	8000.424539	12.614195	-0.052760	4.815725
256.896585	8000.441702	12.619200	-0.052725	4.815731
257.035724	8000.409788	12.624205	-0.052750	4.815721
257.112642	8000.430249	12.629210	-0.052765	4.815727
257.137253	8000.432775	12.634215	-0.052769	4.815727
257.018073	8000.446843	12.639219	-0.052747	4.815732
256.944004	8000.476593	12.644224	-0.052733	4.815741
256.818641	8000.400870	12.649229	-0.052709	4.815720
256.980755	8000.429123	12.654234	-0.052739	4.815727
257.014377	8000.431796	12.659239	-0.052746	4.815728
257.179291	8000.453688	12.664243	-0.052776	4.815733
257.246284	8000.428074	12.669248	-0.052789	4.815725
257.031148	8000.409617	12.674253	-0.052748	4.815721
256.832626	8000.442681	12.679258	-0.052711	4.815732
256.986989	8000.432369	12.684263	-0.052740	4.815728
257.047912	8000.426944	12.689267	-0.052751	4.815726
257.115411	8000.458997	12.694272	-0.052764	4.815735
257.234648	8000.379778	12.699277	-0.052786	4.815711
257.073665	8000.450824	12.704282	-0.052756	4.815733
257.034834	8000.405338	12.709287	-0.052748	4.815720
257.176597	8000.439666	12.714291	-0.052775	4.815729
257.098285	8000.491770	12.719296	-0.052760	4.815745
256.804787	8000.414380	12.724301	-0.052705	4.815724
257.285877	8000.454228	12.729306	-0.052795	4.815733
257.174919	8000.417178	12.734311	-0.052774	4.815723
256.909759	8000.402178	12.739315	-0.052724	4.815720
256.820451	8000.444493	12.744320	-0.052708	4.815732
257.137792	8000.389851	12.749325	-0.052767	4.815715
257.244287	8000.455639	12.754330	-0.052786	4.815734
257.048971	8000.358490	12.759335	-0.052750	4.815706
256.984011	8000.390524	12.764339	-0.052738	4.815716
257.028007	8000.438211	12.769344	-0.052746	4.815729
256.969023	8000.387058	12.774349	-0.052735	4.815715
256.994016	8000.430164	12.779354	-0.052739	4.815727
256.930425	8000.392817	12.784359	-0.052727	4.815717
256.792032	8000.432198	12.789363	-0.052701	4.815729
256.931639	8000.423782	12.794368	-0.052727	4.815726
257.012696	8000.369568	12.799373	-0.052742	4.815710
256.990658	8000.414045	12.804378	-0.052738	4.815723
256.873476	8000.396113	12.809383	-0.052716	4.815718
256.958538	8000.410300	12.814387	-0.052732	4.815722
256.890239	8000.400637	12.819392	-0.052719	4.815719
256.855970	8000.361632	12.824397	-0.052712	4.815708
256.926744	8000.438583	12.829402	-0.052726	4.815730
257.058439	8000.422563	12.834407	-0.052750	4.815725
256.974030	8000.405165	12.839411	-0.052734	4.815720
256.828305	8000.405988	12.844416	-0.052707	4.815721
256.997649	8000.396988	12.849421	-0.052738	4.815718
257.058790	8000.441750	12.854426	-0.052750	4.815730
256.953508	8000.384505	12.859431	-0.052730	4.815714
257.003676	8000.435495	12.864435	-0.052739	4.815729
257.179506	8000.452226	12.869440	-0.052772	4.815733
256.992828	8000.379777	12.874445	-0.052737	4.815713
257.056105	8000.465148	12.879450	-0.052749	4.815737
256.843294	8000.418967	12.884455	-0.052709	4.815725
256.975697	8000.425382	12.889459	-0.052733	4.815726
256.943648	8000.485713	12.894464	-0.052727	4.815744
256.873923	8000.411962	12.899469	-0.052714	4.815723
257.094254	8000.401655	12.904474	-0.052755	4.815719
256.883317	8000.373657	12.909479	-0.052716	4.815711
256.968712	8000.419881	12.914483	-0.052731	4.815724
257.126351	8000.484365	12.919488	-0.052761	4.815743
257.121351	8000.436225	12.924493	-0.052760	4.815729
257.085110	8000.444168	12.929498	-0.052753	4.815731
257.056040	8000.424466	12.934503	-0.052747	4.815725
257.222734	8000.401542	12.939507	-0.052778	4.815718
257.248108	8000.410487	12.944512	-0.052783	4.815720
257.141693	8000.385256	12.949517	-0.052763	4.815714
257.183620	8000.425435	12.954522	-0.052771	4.815725
257.283850	8000.409972	12.959527	-0.052789	4.815720
257.060402	8000.393514	12.964531	-0.052747	4.815716
257.119784	8000.469213	12.969536	-0.052758	4.815738
257.218542	8000.380051	12.974541	-0.052777	4.815712
257.254987	8000.429751	12.979546	-0.052783	4.815726
257.360777	8000.404768	12.984551	-0.052803	4.815718
257.153071	8000.382160	12.989555	-0.052764	4.815713
257.218870	8000.413118	12.994560	-0.052776	4.815721
257.123765	8000.390206	12.999565	-0.052758	4.815715
257.415539	8000.477160	13.004570	-0.052813	4.815739
257.294143	8000.405771	13.009575	-0.052790	4.815719
257.087447	8000.431229	13.014579	-0.052751	4.815727
257.390840	8000.431883	13.019584	-0.052808	4.815726
257.224767	8000.385394	13.024589	-0.052777	4.815713
257.296836	8000.436741	13.029594	-0.052790	4.815728
257.110416	8000.470002	13.034599	-0.052755	4.815739
257.066986	8000.398815	13.039603	-0.052747	4.815718
256.987340	8000.427407	13.044608	-0.052732	4.815727
257.146003	8000.356303	13.049613	-0.052761	4.815705
257.280978	8000.406538	13.054618	-0.052786	4.815719
257.251039	8000.350518	13.059623	-0.052781	4.815703
257.085165	8000.389452	13.064627	-0.052750	4.815715
257.326117	8000.430733	13.069632	-0.052795	4.815726
257.277196	8000.371202	13.074637	-0.052785	4.815709
257.318442	8000.396421	13.079642	-0.052793	4.815716
257.324340	8000.393304	13.084647	-0.052794	4.815715
257.303211	8000.424983	13.089651	-0.052790	4.815724
257.276158	8000.480057	13.094656	-0.052785	4.815741
257.117649	8000.390981	13.099661	-0.052755	4.815715
257.349847	8000.403290	13.104666	-0.052798	4.815718
257.331420	8000.389100	13.109671	-0.052795	4.815714
257.206499	8000.419091	13.114675	-0.052771	4.815723
257.098074	8000.406640	13.119680	-0.052751	4.815720
257.191040	8000.385720	13.124685	-0.052768	4.815714
257.120571	8000.472119	13.129690	-0.052755	4.815739
256.951007	8000.450132	13.134695	-0.052723	4.815734
257.143779	8000.431903	13.139699	-0.052759	4.815727
257.179489	8000.429271	13.144704	-0.052766	4.815726
257.247253	8000.363095	13.149709	-0.052778	4.815707
257.180819	8000.449560	13.154714	-0.052766	4.815732
257.392127	8000.397465	13.159719	-0.052805	4.815716
257.256585	8000.415537	13.164723	-0.052780	4.815722
257.198197	8000.426323	13.169728	-0.052769	4.815725
257.185323	8000.397275	13.174733	-0.052766	4.815717
257.146062	8000.444675	13.179738	-0.052759	4.815731
257.104316	8000.423699	13.184743	-0.052751	4.815725
257.138751	8000.441334	13.189747	-0.052757	4.815730
257.228460	8000.459867	13.194752	-0.052774	4.815735
257.115458	8000.370464	13.199757	-0.052752	4.815710
257.153407	8000.416985	13.204762	-0.052759	4.815723
256.977885	8000.413053	13.209767	-0.052727	4.815723
257.151499	8000.389173	13.214771	-0.052759	4.815715
257.283899	8000.478873	13.219776	-0.052783	4.815740
257.305460	8000.424758	13.224781	-0.052787	4.815724
257.345246	8000.515087	13.229786	-0.052795	4.815751
257.390125	8000.467759	13.234791	-0.052803	4.815737
257.255586	8000.438866	13.239795	-0.052778	4.815729
257.236261	8000.456694	13.244800	-0.052774	4.815734
256.933965	8000.422938	13.249805	-0.052718	4.815726
257.007556	8000.465768	13.254810	-0.052731	4.815738
257.131445	8000.389827	13.259815	-0.052754	4.815715
257.022683	8000.368829	13.264819	-0.052734	4.815710
257.042130	8000.402236	13.269824	-0.052737	4.815719
257.084958	8000.379433	13.274829	-0.052745	4.815712
257.217081	8000.398656	13.279834	-0.052770	4.815717
257.055731	8000.432325	13.284839	-0.052739	4.815728
257.064811	8000.411108	13.289843	-0.052741	4.815722
257.215529	8000.416753	13.294848	-0.052769	4.815723
257.003264	8000.401546	13.299853	-0.052729	4.815719
257.132243	8000.428192	13.304858	-0.052753	4.815726
257.186213	8000.470703	13.309863	-0.052763	4.815739
256.879284	8000.428329	13.314867	-0.052706	4.815728
257.007701	8000.443221	13.319872	-0.052730	4.815731
257.155429	8000.419989	13.324877	-0.052757	4.815724
257.084073	8000.445512	13.329882	-0.052744	4.815732
257.042263	8000.367945	13.334887	-0.052736	4.815709
257.192855	8000.402416	13.339891	-0.052764	4.815719
257.176898	8000.401079	13.344896	-0.052761	4.815718
257.044177	8000.376489	13.349901	-0.052736	4.815712
257.227320	8000.422167	13.354906	-0.052770	4.815724
257.508087	8000.367999	13.359911	-0.052822	4.815707
257.189059	8000.391629	13.364915	-0.052762	4.815715
257.082562	8000.404835	13.369920	-0.052743	4.815720
256.955867	8000.395291	13.374925	-0.052719	4.815718
257.136857	8000.397157	13.379930	-0.052752	4.815717
257.056209	8000.397971	13.384935	-0.052737	4.815718
257.012547	8000.385506	13.389939	-0.052729	4.815715
257.305544	8000.414820	13.394944	-0.052784	4.815722
257.134348	8000.372519	13.399949	-0.052752	4.815710
257.280561	8000.378091	13.404954	-0.052779	4.815711
257.220174	8000.398454	13.409959	-0.052767	4.815717
257.299835	8000.428570	13.414963	-0.052782	4.815726
257.218222	8000.428300	13.419968	-0.052767	4.815726
257.429219	8000.390080	13.424973	-0.052806	4.815714
257.532274	8000.435525	13.429978	-0.052825	4.815727
257.391272	8000.411866	13.434983	-0.052799	4.815720
257.321099	8000.428867	13.439987	-0.052785	4.815726
257.410165	8000.459136	13.444992	-0.052802	4.815734
257.271311	8000.405615	13.449997	-0.052776	4.815719
257.202125	8000.432241	13.455002	-0.052763	4.815727
257.172654	8000.369823	13.460007	-0.052757	4.815709
257.312995	8000.368893	13.465011	-0.052783	4.815708
257.442045	8000.420099	13.470016	-0.052807	4.815723
257.371647	8000.411470	13.475021	-0.052794	4.815720
257.502512	8000.415724	13.480026	-0.052818	4.815721
257.375825	8000.418993	13.485031	-0.052795	4.815723
257.409379	8000.366141	13.490035	-0.052801	4.815707
257.618846	8000.450688	13.495040	-0.052840	4.815731
257.173426	8000.395384	13.500045	-0.052757	4.815717
257.245205	8000.409355	13.505050	-0.052770	4.815720
257.220506	8000.428163	13.510055	-0.052765	4.815726
257.214814	8000.390689	13.515059	-0.052764	4.815715
257.363771	8000.495607	13.520064	-0.052792	4.815745
257.214389	8000.418425	13.525069	-0.052764	4.815723
257.204824	8000.432140	13.530074	-0.052762	4.815727
257.194806	8000.410612	13.535079	-0.052760	4.815721
257.380037	8000.421090	13.540083	-0.052794	4.815723
257.367452	8000.459315	13.545088	-0.052792	4.815734
257.197330	8000.424505	13.550093	-0.052760	4.815725
257.293110	8000.422850	13.555098	-0.052778	4.815724
257.275996	8000.452459	13.560103	-0.052774	4.815733
257.341238	8000.380904	13.565107	-0.052786	4.815712
257.270136	8000.386144	13.570112	-0.052773	4.815714
257.337623	8000.316761	13.575117	-0.052785	4.815693
257.534437	8000.371204	13.580122	-0.052822	4.815708
257.469062	8000.409638	13.585127	-0.052810	4.815720
257.449651	8000.399703	13.590131	-0.052806	4.815717
257.658171	8000.462880	13.595136	-0.052845	4.815734
257.738389	8000.386229	13.600141	-0.052860	4.815711
257.565180	8000.395146	13.605146	-0.052827	4.815715
257.493532	8000.414259	13.610151	-0.052814	4.815721
257.464095	8000.394550	13.615155	-0.052808	4.815715
257.548824	8000.451442	13.620160	-0.052824	4.815731
257.566836	8000.400473	13.625165	-0.052827	4.815716
257.624062	8000.388582	13.630170	-0.052838	4.815713
257.482892	8000.412969	13.635175	-0.052811	4.815720
257.304993	8000.399388	13.640179	-0.052778	4.815717
257.568608	8000.380176	13.645184	-0.052827	4.815710
257.664041	8000.477817	13.650189	-0.052845	4.815739
257.551178	8000.438600	13.655194	-0.052824	4.815728
257.481936	8000.451344	13.660199	-0.052811	4.815732
257.589475	8000.406103	13.665203	-0.052830	4.815718
257.686568	8000.433299	13.670208	-0.052848	4.815725
257.403646	8000.380638	13.675213	-0.052796	4.815711
257.513494	8000.424057	13.680218	-0.052816	4.815724
257.625232	8000.458966	13.685223	-0.052837	4.815733
257.587793	8000.427382	13.690227	-0.052830	4.815724
257.630626	8000.523100	13.695232	-0.052837	4.815752
257.496547	8000.392778	13.700237	-0.052812	4.815715
257.522666	8000.420955	13.705242	-0.052817	4.815723
257.477619	8000.414874	13.710247	-0.052809	4.815721
257.599172	8000.399757	13.715251	-0.052831	4.815716
257.575345	8000.431393	13.720256	-0.052827	4.815725
257.350060	8000.386076	13.725261	-0.052784	4.815713
257.471592	8000.407263	13.730266	-0.052807	4.815719
257.533091	8000.424270	13.735271	-0.052818	4.815724
257.314023	8000.414290	13.740275	-0.052777	4.815722
257.607214	8000.425456	13.745280	-0.052832	4.815724
257.554357	8000.397893	13.750285	-0.052822	4.815716
257.553392	8000.417087	13.755290	-0.052822	4.815721
257.341947	8000.384808	13.760295	-0.052782	4.815713
257.447820	8000.418553	13.765299	-0.052802	4.815722
257.598370	8000.502143	13.770304	-0.052830	4.815746
257.444112	8000.396051	13.775309	-0.052801	4.815716
257.487700	8000.418105	13.780314	-0.052809	4.815722
257.546187	8000.397692	13.785319	-0.052820	4.815716
257.451101	8000.384390	13.790323	-0.052802	4.815712
257.510336	8000.389615	13.795328	-0.052813	4.815714
257.404123	8000.344100	13.800333	-0.052793	4.815701
257.764278	8000.437505	13.805338	-0.052860	4.815726
257.356992	8000.399905	13.810343	-0.052784	4.815717
257.317065	8000.375755	13.815347	-0.052776	4.815710
257.431333	8000.398959	13.820352	-0.052798	4.815717
257.358360	8000.377475	13.825357	-0.052784	4.815711
257.481991	8000.405102	13.830362	-0.052807	4.815718
257.732927	8000.385684	13.835367	-0.052853	4.815711
257.346165	8000.367638	13.840371	-0.052781	4.815708
257.414083	8000.407172	13.845376	-0.052794	4.815719
257.620391	8000.391299	13.850381	-0.052832	4.815714
257.592881	8000.427145	13.855386	-0.052827	4.815724
257.448140	8000.401290	13.860391	-0.052800	4.815717
257.412187	8000.386815	13.865395	-0.052793	4.815713
257.497025	8000.412744	13.870400	-0.052809	4.815720
257.350435	8000.361233	13.875405	-0.052781	4.815706
257.556017	8000.388058	13.880410	-0.052819	4.815713
257.535996	8000.417620	13.885415	-0.052816	4.815722
257.578832	8000.392681	13.890419	-0.052823	4.815714
257.493779	8000.401965	13.895424	-0.052807	4.815717
257.641054	8000.358438	13.900429	-0.052835	4.815704
257.722774	8000.391790	13.905434	-0.052850	4.815713
257.749166	8000.379397	13.910439	-0.052855	4.815710
257.702015	8000.360468	13.915443	-0.052846	4.815704
257.862116	8000.387621	13.920448	-0.052876	4.815711
257.475066	8000.384518	13.925453	-0.052803	4.815712
257.508262	8000.396794	13.930458	-0.052809	4.815716
257.613046	8000.487113	13.935463	-0.052829	4.815742
257.537917	8000.400460	13.940467	-0.052815	4.815717
257.647511	8000.411843	13.945472	-0.052835	4.815720
257.613276	8000.400599	13.950477	-0.052829	4.815716
257.581091	8000.409676	13.955482	-0.052822	4.815719
257.539813	8000.449569	13.960487	-0.052815	4.815731
257.508037	8000.379639	13.965491	-0.052809	4.815711
257.626470	8000.402910	13.970496	-0.052831	4.815717
257.499374	8000.373072	13.975501	-0.052807	4.815709
257.515729	8000.398954	13.980506	-0.052810	4.815716
257.511924	8000.443728	13.985511	-0.052809	4.815729
257.379129	8000.395645	13.990515	-0.052784	4.815716
257.508036	8000.397732	13.995520	-0.052808	4.815716
257.729467	8000.357547	14.000525	-0.052849	4.815703
257.614071	8000.383421	14.005530	-0.052827	4.815711
257.760306	8000.367639	14.010535	-0.052855	4.815706
257.709615	8000.387092	14.015539	-0.052845	4.815712
257.754357	8000.424114	14.020544	-0.052853	4.815723
257.639966	8000.387007	14.025549	-0.052832	4.815712
257.649630	8000.386087	14.030554	-0.052833	4.815712
257.757206	8000.404911	14.035559	-0.052853	4.815717
257.597305	8000.406571	14.040563	-0.052824	4.815718
257.676367	8000.420661	14.045568	-0.052838	4.815722
257.645568	8000.385982	14.050573	-0.052832	4.815712
257.757223	8000.414483	14.055578	-0.052853	4.815720
257.747606	8000.413249	14.060583	-0.052851	4.815720
257.580088	8000.345381	14.065587	-0.052820	4.815700
257.881843	8000.395126	14.070592	-0.052876	4.815714
257.692070	8000.428333	14.075597	-0.052840	4.815724
257.712691	8000.425455	14.080602	-0.052844	4.815723
257.821214	8000.435753	14.085607	-0.052864	4.815726
257.648461	8000.396629	14.090611	-0.052832	4.815715
257.544210	8000.456853	14.095616	-0.052812	4.815733
257.576773	8000.410392	14.100621	-0.052818	4.815720
257.736986	8000.427938	14.105626	-0.052848	4.815724
257.638961	8000.445553	14.110631	-0.052830	4.815729
257.565577	8000.384555	14.115635	-0.052816	4.815712
257.640673	8000.454103	14.120640	-0.052830	4.815732
257.539119	8000.409731	14.125645	-0.052811	4.815720
257.626812	8000.420758	14.130650	-0.052827	4.815722
257.841042	8000.416759	14.135655	-0.052867	4.815720
257.838917	8000.393224	14.140659	-0.052866	4.815713
257.736327	8000.442798	14.145664	-0.052847	4.815728
257.658302	8000.375318	14.150669	-0.052832	4.815709
257.719023	8000.435023	14.155674	-0.052844	4.815726
257.683580	8000.477147	14.160679	-0.052837	4.815739
257.594372	8000.400943	14.165683	-0.052820	4.815717
257.799229	8000.462993	14.170688	-0.052858	4.815734
257.701230	8000.450711	14.175693	-0.052840	4.815731
257.608513	8000.449193	14.180698	-0.052823	4.815731
257.849120	8000.461640	14.185703	-0.052867	4.815733
257.744460	8000.406539	14.190707	-0.052848	4.815718
257.719544	8000.434954	14.195712	-0.052843	4.815726
257.727804	8000.438282	14.200717	-0.052844	4.815727
257.784412	8000.415702	14.205722	-0.052855	4.815720
257.731997	8000.478905	14.210727	-0.052845	4.815739
257.720582	8000.384747	14.215731	-0.052843	4.815711
257.738532	8000.419198	14.220736	-0.052846	4.815721
257.829877	8000.419606	14.225741	-0.052863	4.815721
257.863877	8000.434031	14.230746	-0.052869	4.815725
257.917697	8000.451981	14.235751	-0.052879	4.815730
257.832034	8000.448442	14.240755	-0.052863	4.815729
257.737595	8000.444760	14.245760	-0.052845	4.815729
257.724160	8000.471226	14.250765	-0.052843	4.815737
257.787583	8000.417792	14.255770	-0.052854	4.815721
257.896436	8000.446248	14.260775	-0.052874	4.815729
257.796080	8000.426453	14.265779	-0.052856	4.815723
258.037873	8000.481631	14.270784	-0.052901	4.815738
257.804119	8000.408413	14.275789	-0.052857	4.815718
257.947254	7999.347273	14.280794	-0.052883	4.815407

257.919064	7996.201679	14.285799	-0.052875	4.814487
257.812560	7990.640348	14.290803	-0.052852	4.812861
257.685385	7983.918940	14.295808	-0.052824	4.810895
257.461109	7976.653960	14.300813	-0.052777	4.808769
257.536600	7969.028190	14.305818	-0.052786	4.806535
257.743506	7961.243915	14.310823	-0.052819	4.804253
257.439071	7953.348000	14.315827	-0.052757	4.801940
257.535146	7945.409851	14.320832	-0.052770	4.799611
257.537894	7937.451815	14.325837	-0.052765	4.797276
257.388153	7929.408265	14.330842	-0.052732	4.794915
257.385535	7921.381482	14.335847	-0.052726	4.792557
257.683672	7913.377787	14.340851	-0.052776	4.790204
257.531630	7905.415156	14.345856	-0.052743	4.787863
257.395003	7897.374998	14.350861	-0.052712	4.785499
257.229336	7889.397869	14.355866	-0.052676	4.783152
257.210693	7881.428816	14.360871	-0.052667	4.780805
257.134774	7873.408903	14.365875	-0.052647	4.778443
257.163897	7865.430364	14.370880	-0.052648	4.776091
257.040951	7857.358548	14.375885	-0.052619	4.773711
256.930736	7849.354446	14.380890	-0.052593	4.771350
256.960731	7841.396278	14.385895	-0.052594	4.769001
257.150963	7833.428135	14.390899	-0.052624	4.766647
257.030078	7825.441108	14.395904	-0.052596	4.764287
256.762460	7817.393010	14.400909	-0.052541	4.761909
257.007118	7809.339179	14.405914	-0.052581	4.759526
257.069749	7801.397959	14.410919	-0.052587	4.757175
256.953789	7793.336351	14.415923	-0.052560	4.754789
256.730794	7785.346148	14.420928	-0.052514	4.752423
256.858199	7777.289054	14.425933	-0.052532	4.750034
256.723523	7769.350014	14.430938	-0.052502	4.747681
256.664949	7761.314770	14.435943	-0.052485	4.745297
256.534590	7753.317556	14.440947	-0.052456	4.742924
256.560571	7745.353309	14.445952	-0.052455	4.740559
256.305025	7737.321966	14.450957	-0.052402	4.738173
256.337691	7729.341670	14.455962	-0.052403	4.735801
256.538016	7721.349125	14.460967	-0.052435	4.733423
256.243203	7713.294028	14.465971	-0.052375	4.731027
256.440208	7705.322056	14.470976	-0.052406	4.728653
256.348030	7697.329433	14.475981	-0.052384	4.726272
256.289336	7689.290903	14.480986	-0.052367	4.723877
256.142072	7681.340514	14.485991	-0.052335	4.721507
256.026220	7673.300282	14.490995	-0.052308	4.719108
256.285968	7665.373918	14.496000	-0.052351	4.716742
256.260326	7657.286119	14.501005	-0.052341	4.714327
256.163439	7649.268788	14.506010	-0.052317	4.711931
256.370823	7641.288163	14.511015	-0.052351	4.709545
256.144452	7633.289526	14.516019	-0.052303	4.707153
256.051414	7625.317912	14.521024	-0.052281	4.704768
256.007928	7617.350732	14.526029	-0.052267	4.702383
256.130813	7609.305393	14.531034	-0.052285	4.699973
256.000407	7601.336411	14.536039	-0.052255	4.697585
255.904796	7593.298900	14.541043	-0.052232	4.695175
255.975038	7585.279076	14.546048	-0.052240	4.692769
255.967541	7577.269119	14.551053	-0.052233	4.690365
255.790493	7569.302824	14.556058	-0.052195	4.687972
255.810003	7561.271144	14.561063	-0.052193	4.685559
255.782683	7553.198704	14.566067	-0.052183	4.683132
255.980080	7545.369282	14.571072	-0.052214	4.680777
255.881038	7537.331685	14.576077	-0.052190	4.678359
255.831772	7529.294388	14.581082	-0.052176	4.675939
255.919565	7521.252595	14.586087	-0.052187	4.673516
255.729377	7513.125680	14.591091	-0.052146	4.671067
255.896030	7505.187835	14.596096	-0.052172	4.668673
255.561080	7497.200231	14.601101	-0.052104	4.666263
255.451915	7489.240517	14.606106	-0.052078	4.663861
255.437043	7481.279104	14.611111	-0.052070	4.661456
255.536600	7473.222026	14.616115	-0.052084	4.659021
255.435541	7465.259311	14.621120	-0.052059	4.656614
255.401288	7457.221521	14.626125	-0.052048	4.654182
255.411781	7449.213866	14.631130	-0.052044	4.651759
255.389261	7441.214422	14.636135	-0.052035	4.649336
255.278104	7433.225120	14.641139	-0.052009	4.646916
255.570983	7425.226566	14.646144	-0.052058	4.644491
255.547960	7417.243753	14.651149	-0.052048	4.642070
255.533200	7409.205483	14.656154	-0.052040	4.639631
255.592287	7401.311395	14.661159	-0.052046	4.637234
255.273431	7393.179321	14.666163	-0.051981	4.634764
255.236898	7385.186632	14.671168	-0.051969	4.632335
255.272359	7377.178743	14.676173	-0.051970	4.629899
255.368471	7369.185380	14.681178	-0.051983	4.627467
255.336000	7361.162253	14.686183	-0.051972	4.625025
254.977479	7353.180080	14.691187	-0.051900	4.622594
255.328679	7345.188207	14.696192	-0.051960	4.620158
254.919294	7337.202301	14.701197	-0.051878	4.617724
255.094619	7329.159401	14.706202	-0.051905	4.615270
255.047740	7321.203587	14.711207	-0.051891	4.612842
254.938117	7313.120167	14.716211	-0.051866	4.610373
254.908525	7305.195329	14.721216	-0.051855	4.607952
254.801916	7297.178765	14.726221	-0.051830	4.605501
254.903993	7289.165300	14.731226	-0.051843	4.603050
255.012252	7281.196861	14.736231	-0.051858	4.600611
254.821568	7273.166755	14.741235	-0.051817	4.598152
255.015289	7265.197492	14.746240	-0.051848	4.595711
254.693864	7257.163025	14.751245	-0.051783	4.593248
254.606293	7249.059281	14.756250	-0.051761	4.590763
254.996775	7241.138993	14.761255	-0.051829	4.588332
254.726003	7233.101272	14.766259	-0.051773	4.585865
254.653278	7225.134556	14.771264	-0.051754	4.583417
254.615560	7217.121263	14.776269	-0.051742	4.580954
254.508102	7209.160207	14.781274	-0.051716	4.578506
254.465118	7201.176886	14.786279	-0.051703	4.576050
254.279179	7193.101015	14.791283	-0.051663	4.573563
254.399928	7185.126845	14.796288	-0.051680	4.571107
254.414986	7177.124900	14.801293	-0.051678	4.568641
254.288004	7169.135923	14.806298	-0.051649	4.566178
254.311263	7161.170942	14.811303	-0.051648	4.563720
254.480609	7153.129753	14.816307	-0.051674	4.561238
254.436785	7145.139304	14.821312	-0.051660	4.558770
254.250579	7137.154875	14.826317	-0.051620	4.556303
254.307480	7129.129266	14.831322	-0.051626	4.553821
254.313232	7121.121389	14.836327	-0.051621	4.551344
254.077851	7113.107034	14.841331	-0.051572	4.548863
254.347275	7105.110552	14.846336	-0.051617	4.546387
254.223002	7097.103407	14.851341	-0.051589	4.543905
254.010160	7089.109259	14.856346	-0.051544	4.541427
254.135556	7081.154773	14.861351	-0.051562	4.538959
254.043808	7073.121442	14.866355	-0.051539	4.536466
253.873461	7065.149355	14.871360	-0.051502	4.533990
253.808800	7057.086583	14.876365	-0.051485	4.531484
253.936954	7049.085229	14.881370	-0.051503	4.528997
253.770188	7041.115363	14.886375	-0.051467	4.526517
253.865035	7033.056813	14.891379	-0.051479	4.524010
254.011846	7025.151660	14.896384	-0.051501	4.521548
253.952946	7017.142121	14.901389	-0.051485	4.519052
253.895468	7009.123010	14.906394	-0.051469	4.516552
253.876189	7001.111071	14.911399	-0.051460	4.514053
253.970709	6993.018658	14.916403	-0.051472	4.511528
253.909968	6985.040982	14.921408	-0.051456	4.509036
253.719052	6977.069851	14.926413	-0.051415	4.506545
253.741918	6969.052433	14.931418	-0.051414	4.504039
253.860290	6961.121448	14.936423	-0.051431	4.501559
253.537174	6953.061180	14.941427	-0.051365	4.499035
253.534326	6945.070377	14.946432	-0.051359	4.496533
253.549990	6937.074892	14.951437	-0.051357	4.494028
253.621748	6929.018611	14.956442	-0.051365	4.491502
253.564592	6921.034779	14.961447	-0.051349	4.488998
253.520034	6913.059285	14.966451	-0.051335	4.486495
253.439521	6905.049874	14.971456	-0.051315	4.483979
253.374947	6897.089531	14.976461	-0.051298	4.481478
253.396819	6889.019570	14.981466	-0.051296	4.478941
253.449213	6881.136422	14.986471	-0.051301	4.476461
253.441834	6873.025241	14.991475	-0.051294	4.473909
253.429995	6865.020837	14.996480	-0.051286	4.471388
253.394965	6856.995469	15.001485	-0.051275	4.468859
253.373465	6849.019059	15.006490	-0.051265	4.466344
253.256225	6841.008710	15.011495	-0.051238	4.463817
253.394793	6833.048342	15.016499	-0.051259	4.461305
253.422877	6825.037422	15.021504	-0.051259	4.458775
253.157854	6817.071218	15.026509	-0.051204	4.456257
253.205214	6809.002051	15.031514	-0.051207	4.453706
253.043228	6801.006270	15.036519	-0.051172	4.451176
252.857284	6793.029224	15.041523	-0.051132	4.448650
253.044056	6785.024297	15.046528	-0.051161	4.446116
253.018194	6776.999126	15.051533	-0.051151	4.443573
252.763422	6769.030884	15.056538	-0.051098	4.441045
252.929230	6761.057581	15.061543	-0.051124	4.438516
252.830989	6753.015746	15.066547	-0.051100	4.435963
253.090797	6744.997121	15.071552	-0.051143	4.433417
252.695303	6736.942294	15.076557	-0.051064	4.430856
252.814501	6728.962368	15.081562	-0.051081	4.428319
252.867215	6720.957544	15.086567	-0.051086	4.425772
252.711851	6712.948646	15.091571	-0.051052	4.423222
252.471829	6705.010384	15.096576	-0.051002	4.420692
252.618458	6697.015045	15.101581	-0.051024	4.418145
252.758355	6688.974458	15.106586	-0.051044	4.415581
252.537515	6681.004787	15.111591	-0.050998	4.413037
252.287474	6672.934694	15.116595	-0.050946	4.410459
252.508240	6664.955662	15.121600	-0.050982	4.407911
252.631518	6656.970054	15.126605	-0.050999	4.405359
252.512322	6648.964718	15.131610	-0.050972	4.402798
252.551378	6640.984871	15.136615	-0.050974	4.400245
252.314890	6633.047424	15.141619	-0.050924	4.397702
252.398230	6625.012787	15.146624	-0.050935	4.395128
252.282641	6617.032014	15.151629	-0.050908	4.392569
252.285456	6608.935178	15.156634	-0.050903	4.389972
252.149734	6601.025479	15.161639	-0.050872	4.387433
252.428504	6592.948803	15.166643	-0.050919	4.384840
252.245341	6585.015259	15.171648	-0.050880	4.382290
252.154590	6576.981839	15.176653	-0.050857	4.379707
252.087105	6569.014865	15.181658	-0.050839	4.377143
252.182935	6560.997205	15.186663	-0.050852	4.374563
252.065004	6552.996975	15.191667	-0.050825	4.371985
251.903725	6544.971351	15.196672	-0.050789	4.369398
252.027193	6537.013820	15.201677	-0.050807	4.366832
252.037006	6528.946081	15.206682	-0.050803	4.364229
251.859537	6521.025056	15.211687	-0.050765	4.361671
251.677470	6513.018032	15.216691	-0.050726	4.359083
251.907093	6505.038541	15.221696	-0.050763	4.356505
251.789892	6496.956798	15.226701	-0.050736	4.353890
251.605600	6488.836965	15.231706	-0.050696	4.351261
251.599520	6480.893882	15.236711	-0.050690	4.348689
251.626953	6472.919176	15.241715	-0.050690	4.346105
251.726296	6464.938080	15.246720	-0.050703	4.343518
251.736278	6456.986682	15.251725	-0.050700	4.340939
251.524614	6448.947616	15.256730	-0.050655	4.338328
251.570868	6440.992508	15.261735	-0.050658	4.335745
251.491037	6432.952668	15.266739	-0.050638	4.333131
251.464735	6424.926146	15.271744	-0.050628	4.330521
251.233844	6416.938728	15.276749	-0.050579	4.327920
251.461819	6408.913414	15.281754	-0.050616	4.325309
251.535907	6401.007448	15.286759	-0.050625	4.322734
251.214487	6392.971500	15.291763	-0.050560	4.320112
251.265704	6384.990433	15.296768	-0.050564	4.317509
251.232670	6376.971160	15.301773	-0.050553	4.314892
251.244537	6368.900301	15.306778	-0.050549	4.312256
251.294761	6360.918489	15.311783	-0.050553	4.309648
251.202757	6352.928624	15.316787	-0.050531	4.307035
251.278870	6344.900541	15.321792	-0.050540	4.304409
251.280302	6336.951584	15.326797	-0.050535	4.301807
251.085593	6328.918810	15.331802	-0.050493	4.299174
251.172492	6321.005113	15.336807	-0.050504	4.296581
251.193640	6312.887468	15.341811	-0.050503	4.293919
251.269426	6304.915212	15.346816	-0.050511	4.291304
251.175652	6296.952024	15.351821	-0.050489	4.288688
250.963502	6288.924524	15.356826	-0.050444	4.286049
250.844649	6280.963302	15.361831	-0.050416	4.283430
250.935772	6272.898234	15.366835	-0.050428	4.280778
250.990597	6264.949052	15.371840	-0.050433	4.278161
250.743368	6256.936743	15.376845	-0.050382	4.275520
250.735039	6248.894846	15.381850	-0.050375	4.272870
250.661043	6240.879553	15.386855	-0.050356	4.270226
250.813118	6232.892589	15.391859	-0.050379	4.267591
250.840026	6224.880764	15.396864	-0.050378	4.264946
250.848063	6216.938647	15.401869	-0.050374	4.262322
250.756611	6208.895558	15.406874	-0.050352	4.259662
250.746470	6200.937398	15.411879	-0.050345	4.257029
250.521942	6192.898606	15.416883	-0.050298	4.254366
250.704708	6184.863103	15.421888	-0.050326	4.251706
250.682440	6176.911723	15.426893	-0.050317	4.249071
250.570736	6168.868989	15.431898	-0.050291	4.246402
250.696288	6160.914950	15.436903	-0.050309	4.243764
250.555297	6152.931099	15.441907	-0.050277	4.241111
250.599930	6144.937600	15.446912	-0.050280	4.238456
250.347396	6136.958603	15.451917	-0.050228	4.235801
250.176428	6128.939200	15.456922	-0.050191	4.233131
250.345879	6120.905616	15.461927	-0.050217	4.230458
250.105148	6112.960314	15.466931	-0.050167	4.227809
250.177881	6104.902205	15.471936	-0.050175	4.225124
250.135545	6096.965851	15.476941	-0.050162	4.222477
250.236674	6088.893664	15.481946	-0.050175	4.219783
250.424535	6080.981922	15.486951	-0.050205	4.217143
250.262039	6072.937203	15.491955	-0.050169	4.214453
250.232460	6064.926301	15.496960	-0.050159	4.211774
250.148849	6056.918446	15.501965	-0.050138	4.209094
250.046572	6048.929362	15.506970	-0.050113	4.206418
250.097682	6040.963925	15.511975	-0.050118	4.203750
249.930199	6032.929385	15.516979	-0.050081	4.201055
249.973527	6024.949253	15.521984	-0.050084	4.198378
249.994701	6016.973974	15.526989	-0.050082	4.195702
249.844902	6008.827119	15.531994	-0.050049	4.192964
249.874481	6000.815468	15.536999	-0.050049	4.190271
249.773339	5992.861440	15.542003	-0.050025	4.187595
249.753818	5984.888564	15.547008	-0.050016	4.184912
249.879393	5976.935536	15.552013	-0.050034	4.182235
249.806178	5968.854237	15.557018	-0.050015	4.179511
249.757973	5960.940323	15.562023	-0.050001	4.176842
249.790641	5952.884503	15.567027	-0.050002	4.174124
249.682652	5944.910734	15.572032	-0.049976	4.171431
249.585016	5936.920571	15.577037	-0.049953	4.168730
249.469859	5928.876219	15.582042	-0.049926	4.166009
249.406797	5920.933198	15.587047	-0.049909	4.163322
249.554746	5912.919888	15.592051	-0.049931	4.160611
249.645345	5904.914644	15.597056	-0.049943	4.157900
249.395513	5896.934665	15.602061	-0.049891	4.155193
249.466083	5888.866025	15.607066	-0.049899	4.152457
249.766459	5880.866363	15.612071	-0.049949	4.149745
249.544819	5872.885597	15.617075	-0.049903	4.147032
249.436753	5864.873989	15.622080	-0.049877	4.144308
249.359529	5856.950119	15.627085	-0.049858	4.141613
249.359711	5848.871842	15.632090	-0.049852	4.138864
249.377682	5840.890871	15.637095	-0.049850	4.136147
249.364581	5832.895203	15.642099	-0.049843	4.133422
249.296915	5824.852799	15.647104	-0.049825	4.130679
249.403010	5816.889003	15.652109	-0.049839	4.127963
249.241325	5808.874435	15.657114	-0.049804	4.125225
249.296087	5800.965976	15.662119	-0.049809	4.122524
248.936361	5792.916492	15.667123	-0.049736	4.119767
249.004681	5784.951450	15.672128	-0.049744	4.117043
249.245046	5776.896768	15.677133	-0.049783	4.114289
248.960081	5768.849894	15.682138	-0.049725	4.111529
249.019416	5760.884721	15.687143	-0.049730	4.108799
249.066462	5752.845225	15.692147	-0.049734	4.106042
248.913498	5744.884243	15.697152	-0.049700	4.103308
248.632755	5736.910842	15.702157	-0.049642	4.100565
248.663115	5728.900897	15.707162	-0.049643	4.097813
249.006338	5720.905036	15.712167	-0.049701	4.095067
248.851594	5712.868570	15.717171	-0.049667	4.092299
248.585449	5704.893642	15.722176	-0.049612	4.089549
248.708438	5696.945968	15.727181	-0.049630	4.086812
248.610521	5688.901024	15.732186	-0.049606	4.084036
248.665505	5680.966741	15.737191	-0.049611	4.081299
248.622555	5672.935949	15.742195	-0.049598	4.078525
248.690268	5664.957672	15.747200	-0.049605	4.075769
248.537648	5656.920574	15.752205	-0.049571	4.072987
248.352580	5648.880435	15.757210	-0.049532	4.070202
248.389257	5640.966617	15.762215	-0.049533	4.067463
248.418802	5632.912507	15.767219	-0.049533	4.064672
248.290784	5624.964921	15.772224	-0.049504	4.061914
248.356628	5616.959002	15.777229	-0.049511	4.059137
248.278823	5608.946540	15.782234	-0.049491	4.056354
248.392936	5600.952257	15.787239	-0.049507	4.053578
248.234672	5592.911116	15.792243	-0.049472	4.050780
248.249820	5584.928388	15.797248	-0.049470	4.048002
248.083645	5576.916693	15.802253	-0.049434	4.045210
247.875759	5568.921339	15.807258	-0.049390	4.042422
248.187399	5560.944295	15.812263	-0.049442	4.039645
248.194307	5552.980334	15.817267	-0.049438	4.036866
247.919236	5544.891006	15.822272	-0.049382	4.034038
248.068201	5536.834654	15.827277	-0.049404	4.031225
247.975181	5528.872953	15.832282	-0.049382	4.028440
248.150450	5520.905967	15.837287	-0.049409	4.025655
247.961530	5512.903373	15.842291	-0.049368	4.022850
247.893238	5504.897563	15.847296	-0.049350	4.020044
247.984433	5496.924138	15.852301	-0.049362	4.017250
247.867070	5488.873891	15.857306	-0.049335	4.014424
247.962111	5480.909655	15.862311	-0.049347	4.011629
247.938651	5472.886970	15.867315	-0.049337	4.008810
247.875566	5464.905463	15.872320	-0.049320	4.006002
247.901634	5456.969012	15.877325	-0.049320	4.003210
247.814919	5448.904945	15.882330	-0.049298	4.000370
247.673815	5440.938594	15.887335	-0.049267	3.997561
247.580440	5432.898716	15.892339	-0.049244	3.994724
247.698554	5424.884045	15.897344	-0.049261	3.991898
247.868600	5416.927407	15.902349	-0.049287	3.989092
247.520344	5408.916459	15.907354	-0.049217	3.986255
247.440483	5400.952693	15.912359	-0.049197	3.983438
247.411896	5392.927818	15.917363	-0.049186	3.980598
247.466271	5384.927704	15.922368	-0.049191	3.977766
247.401124	5376.944198	15.927373	-0.049174	3.974936
247.466352	5368.889826	15.932378	-0.049180	3.972081
247.332485	5360.914020	15.937383	-0.049150	3.969248
247.200497	5352.925427	15.942387	-0.049120	3.966409
247.309707	5344.865180	15.947392	-0.049135	3.963546
247.357234	5336.957609	15.952397	-0.049139	3.960735
247.185881	5329.010977	15.957402	-0.049102	3.957904
247.493239	5321.022332	15.962407	-0.049153	3.955064
247.408282	5312.957722	15.967411	-0.049132	3.952188
247.282058	5304.961422	15.972416	-0.049103	3.949334
247.265034	5296.963850	15.977421	-0.049095	3.946480
247.231176	5288.955434	15.982426	-0.049083	3.943619
247.152103	5280.990888	15.987431	-0.049063	3.940770
247.170626	5273.001987	15.992435	-0.049061	3.937913
247.104985	5264.987337	15.997440	-0.049044	3.935043
247.000184	5256.985759	16.002445	-0.049019	3.932175
246.903109	5248.940060	16.007450	-0.048996	3.929289
246.948880	5240.987931	16.012455	-0.048999	3.926437
246.914698	5232.989984	16.017459	-0.048987	3.923565
246.825054	5225.006817	16.022464	-0.048965	3.920695
246.761684	5217.054239	16.027469	-0.048948	3.917835
246.888188	5208.955518	16.032474	-0.048966	3.914923
246.793059	5200.982522	16.037479	-0.048943	3.912051
246.738152	5192.970047	16.042483	-0.048928	3.909163
246.825633	5184.964797	16.047488	-0.048939	3.906278
246.868050	5176.975560	16.052493	-0.048941	3.903395
246.838678	5168.980406	16.057498	-0.048930	3.900507
246.834389	5161.027011	16.062503	-0.048924	3.897633
246.845765	5152.991514	16.067507	-0.048921	3.894727
246.771897	5144.962207	16.072512	-0.048902	3.891820
246.656655	5136.994552	16.077517	-0.048875	3.888931
246.405944	5128.981532	16.082522	-0.048823	3.886022
246.430426	5121.033923	16.087527	-0.048822	3.883139
246.333434	5113.009314	16.092531	-0.048799	3.880224
246.379833	5105.020011	16.097536	-0.048802	3.877323
246.400843	5097.016587	16.102541	-0.048801	3.874413
246.301617	5088.732341	16.107546	-0.048777	3.871397
246.410080	5080.847846	16.112551	-0.048792	3.868528
246.539187	5072.888385	16.117555	-0.048811	3.865631
246.283689	5064.940495	16.122560	-0.048758	3.862727
246.262073	5056.982428	16.127565	-0.048748	3.859822
246.285276	5048.958682	16.132570	-0.048747	3.856892
246.475278	5040.989011	16.137575	-0.048778	3.853983
246.217471	5032.967382	16.142579	-0.048724	3.851044
246.167634	5024.995825	16.147584	-0.048710	3.848125
246.347381	5016.991954	16.152589	-0.048738	3.845197
246.059926	5009.050112	16.157594	-0.048679	3.842279
245.925524	5001.077747	16.162599	-0.048649	3.839351
245.887967	4993.085660	16.167603	-0.048636	3.836416
245.963853	4985.010052	16.172608	-0.048645	3.833450
246.058052	4977.016852	16.177613	-0.048657	3.830512
245.954996	4969.018111	16.182618	-0.048633	3.827567
245.975103	4961.040558	16.187623	-0.048631	3.824629
245.749620	4953.095095	16.192627	-0.048584	3.821695
245.561660	4945.087684	16.197632	-0.048544	3.818738
245.748563	4937.082636	16.202637	-0.048573	3.815786
245.712932	4929.064523	16.207642	-0.048561	3.812823
245.614640	4921.052093	16.212647	-0.048537	3.809859
245.590317	4913.088858	16.217651	-0.048528	3.806911
245.398057	4905.067489	16.222656	-0.048486	3.803937
245.459102	4897.130217	16.227661	-0.048493	3.800996
245.534857	4889.099754	16.232666	-0.048501	3.798020
245.770131	4881.084615	16.237671	-0.048540	3.795050
245.307154	4873.073435	16.242675	-0.048448	3.792063
245.262908	4865.061455	16.247680	-0.048435	3.789084
245.389034	4857.070783	16.252685	-0.048453	3.786114
245.345230	4849.067189	16.257690	-0.048439	3.783132
245.245999	4841.098387	16.262695	-0.048416	3.780161
245.283262	4833.144401	16.267699	-0.048417	3.777195
245.264398	4825.058744	16.272704	-0.048408	3.774177
245.253397	4817.099399	16.277709	-0.048401	3.771203
245.138339	4809.064194	16.282714	-0.048374	3.768197
245.029632	4801.093460	16.287719	-0.048349	3.765212
244.934621	4793.131594	16.292723	-0.048326	3.762229
244.911725	4785.075051	16.297728	-0.048316	3.759209
244.998083	4777.166375	16.302733	-0.048327	3.756245
244.878615	4769.066290	16.307738	-0.048299	3.753202
245.052412	4761.078412	16.312743	-0.048326	3.750206
245.099330	4753.105581	16.317747	-0.048330	3.747209
245.090148	4745.060501	16.322752	-0.048323	3.744182
244.962188	4737.163647	16.327757	-0.048294	3.741206
244.681268	4729.136176	16.332762	-0.048236	3.738174
245.033641	4721.115958	16.337767	-0.048296	3.735157
244.969989	4713.131693	16.342771	-0.048279	3.732142
244.671257	4705.133306	16.347776	-0.048218	3.729114
244.900418	4697.165742	16.352781	-0.048255	3.726107
244.656581	4689.157178	16.357786	-0.048205	3.723071
244.743892	4681.208228	16.362791	-0.048216	3.720063
244.579298	4673.239033	16.367795	-0.048180	3.717038
244.620119	4665.189125	16.372800	-0.048182	3.713986
244.598090	4657.117001	16.377805	-0.048172	3.710921
244.292806	4649.111807	16.382810	-0.048110	3.707872
244.588642	4641.121872	16.387815	-0.048160	3.704841
244.505754	4633.176980	16.392819	-0.048139	3.701816
244.238982	4625.186737	16.397824	-0.048084	3.698766
244.189750	4617.214323	16.402829	-0.048070	3.695726
244.368261	4609.174623	16.407834	-0.048098	3.692663
244.258909	4601.193201	16.412839	-0.048072	3.689613
244.221498	4593.219392	16.417843	-0.048060	3.686565
244.278089	4585.207612	16.422848	-0.048065	3.683502
244.251040	4577.252068	16.427853	-0.048055	3.680456
244.291451	4569.252194	16.432858	-0.048057	3.677393
244.013637	4561.242829	16.437863	-0.048000	3.674315
244.258862	4553.206828	16.442867	-0.048040	3.671237
244.088337	4545.233074	16.447872	-0.048003	3.668171
244.124841	4537.204193	16.452877	-0.048005	3.665085
244.073247	4529.218041	16.457882	-0.047990	3.662012
244.167558	4521.237634	16.462887	-0.048002	3.658942
244.165562	4513.272876	16.467891	-0.047996	3.655872
244.137729	4505.242135	16.472896	-0.047986	3.652774
244.018317	4497.238240	16.477901	-0.047958	3.649682
243.819917	4489.257113	16.482906	-0.047916	3.646593
243.752723	4481.281879	16.487911	-0.047898	3.643508
243.881017	4473.308003	16.492915	-0.047917	3.640425
243.831997	4465.320072	16.497920	-0.047902	3.637330
243.764136	4457.295999	16.502925	-0.047884	3.634218
243.543813	4449.223498	16.507930	-0.047838	3.631080
243.402388	4441.251418	16.512935	-0.047806	3.627980
243.403999	4433.244087	16.517939	-0.047801	3.624868
243.629062	4425.264854	16.522944	-0.047838	3.621771
243.500069	4417.296438	16.527949	-0.047808	3.618665
243.266259	4409.304685	16.532954	-0.047760	3.615544
243.300640	4401.320962	16.537959	-0.047761	3.612432
243.472555	4393.294373	16.542963	-0.047787	3.609304
243.137242	4385.335538	16.547968	-0.047720	3.606185
243.144276	4377.365695	16.552973	-0.047716	3.603069
243.153237	4369.331642	16.557978	-0.047712	3.599925
243.098171	4361.394452	16.562983	-0.047696	3.596815
242.997155	4353.389454	16.567987	-0.047672	3.593674
242.943291	4345.363449	16.572992	-0.047657	3.590523
243.097626	4337.366807	16.577997	-0.047680	3.587387
242.970492	4329.338758	16.583002	-0.047651	3.584228
243.042630	4321.413618	16.588007	-0.047659	3.581112
242.971778	4313.413047	16.593011	-0.047641	3.577960
242.938042	4305.377260	16.598016	-0.047629	3.574792
242.745063	4297.411714	16.603021	-0.047588	3.571644
242.961121	4289.370261	16.608026	-0.047623	3.568476
242.826021	4281.402801	16.613031	-0.047592	3.565323
242.643552	4273.450688	16.618035	-0.047553	3.562173
242.573724	4265.427194	16.623040	-0.047535	3.558995
242.817513	4257.441957	16.628045	-0.047575	3.555838
242.535445	4249.368301	16.633050	-0.047517	3.552628
242.753433	4241.322137	16.638055	-0.047552	3.549441
242.706469	4233.397984	16.643059	-0.047538	3.546291
242.705810	4225.402866	16.648064	-0.047533	3.543112
242.612420	4217.419554	16.653069	-0.047510	3.539932
242.536329	4209.441376	16.658074	-0.047491	3.536752
242.714103	4201.417562	16.663079	-0.047518	3.533558
242.362537	4193.431676	16.668083	-0.047448	3.530360
242.288622	4185.453181	16.673088	-0.047429	3.527171
242.628808	4177.426969	16.678093	-0.047487	3.523973
242.543748	4169.473915	16.683098	-0.047465	3.520788
242.288276	4161.518558	16.688103	-0.047413	3.517594
242.326432	4153.511418	16.693107	-0.047414	3.514385
242.230535	4145.511010	16.698112	-0.047391	3.511172
242.200175	4137.513695	16.703117	-0.047380	3.507959
242.133310	4129.474540	16.708122	-0.047362	3.504725
242.248326	4121.536538	16.713127	-0.047378	3.501535
242.206516	4113.539656	16.718131	-0.047365	3.498313
241.981156	4105.536603	16.723136	-0.047318	3.495080
242.251778	4097.557224	16.728141	-0.047363	3.491869
242.089839	4089.547858	16.733146	-0.047328	3.488629
241.750120	4081.560744	16.738151	-0.047259	3.485389
241.952947	4073.609468	16.743155	-0.047292	3.482179
242.043406	4065.599560	16.748160	-0.047303	3.478938
241.830972	4057.623348	16.753165	-0.047258	3.475698
241.605088	4049.560375	16.758170	-0.047211	3.472419
241.875346	4041.550211	16.763175	-0.047256	3.469175
241.803218	4033.600036	16.768179	-0.047237	3.465941
241.531434	4025.619581	16.773184	-0.047181	3.462685
241.592787	4017.631583	16.778189	-0.047187	3.459433
241.467914	4009.623916	16.783194	-0.047159	3.456165
241.579595	4001.613268	16.788199	-0.047174	3.452900
241.692266	3993.597082	16.793203	-0.047190	3.449630
241.579337	3985.589895	16.798208	-0.047163	3.446353
241.533067	3977.662002	16.803213	-0.047150	3.443107
241.346164	3969.659324	16.808218	-0.047109	3.439823
241.413696	3961.687811	16.813223	-0.047117	3.436557
241.266290	3953.680558	16.818227	-0.047084	3.433266
241.129731	3945.665735	16.823232	-0.047053	3.429969
241.302445	3937.665202	16.828237	-0.047080	3.426685
241.369111	3929.649135	16.833242	-0.047087	3.423389
241.181551	3921.684432	16.838247	-0.047047	3.420101
241.267396	3913.742741	16.843251	-0.047058	3.416829
241.234769	3905.719388	16.848256	-0.047046	3.413517
241.297245	3897.710304	16.853261	-0.047052	3.410210
241.089315	3889.742014	16.858266	-0.047008	3.406907
241.288787	3881.709151	16.863271	-0.047040	3.403589
241.084788	3873.793050	16.868275	-0.046997	3.400302
241.022606	3865.793079	16.873280	-0.046980	3.396981
241.009528	3857.775797	16.878285	-0.046972	3.393653
240.895719	3849.675751	16.883290	-0.046946	3.390282
240.938449	3841.724396	16.888295	-0.046948	3.386976
240.932741	3833.757155	16.893299	-0.046942	3.383658
240.738613	3825.790487	16.898304	-0.046901	3.380331
240.736728	3817.823666	16.903309	-0.046895	3.377007
240.640823	3809.818151	16.908314	-0.046872	3.373660
240.814388	3801.806606	16.913319	-0.046899	3.370317
240.721351	3793.842126	16.918323	-0.046876	3.366981
240.603953	3785.831804	16.923328	-0.046849	3.363621
240.684045	3777.879567	16.928333	-0.046858	3.360290
240.521281	3769.911474	16.933338	-0.046823	3.356940
240.469999	3761.851191	16.938343	-0.046808	3.353551
240.530342	3753.837662	16.943347	-0.046814	3.350183
240.504226	3745.840399	16.948352	-0.046804	3.346816
240.486023	3737.880134	16.953357	-0.046795	3.343460
240.275772	3729.909078	16.958362	-0.046751	3.340090
240.470657	3721.951483	16.963367	-0.046782	3.336737
240.398564	3713.923996	16.968371	-0.046763	3.333341
240.254997	3705.897714	16.973376	-0.046731	3.329940
240.402883	3697.955051	16.978381	-0.046753	3.326581
240.245164	3689.930211	16.983386	-0.046718	3.323173
240.174086	3681.979566	16.988391	-0.046700	3.319796
240.152361	3674.015061	16.993395	-0.046690	3.316411
240.064889	3665.972809	16.998400	-0.046669	3.312988
239.980227	3657.965787	17.003405	-0.046648	3.309576
240.031245	3649.966713	17.008410	-0.046652	3.306169
240.048292	3641.980356	17.013415	-0.046650	3.302762
240.066623	3634.008696	17.018419	-0.046648	3.299359
239.646372	3626.073576	17.023424	-0.046564	3.295950
239.872767	3618.042911	17.028429	-0.046601	3.292522
239.764939	3610.045459	17.033434	-0.046576	3.289092
239.768098	3602.074783	17.038439	-0.046571	3.285674
239.818702	3594.111754	17.043443	-0.046575	3.282258
239.821625	3586.111208	17.048448	-0.046570	3.278820
239.733440	3578.145453	17.053453	-0.046549	3.275390
239.622035	3570.106869	17.058458	-0.046522	3.271924
239.530159	3562.095351	17.063463	-0.046500	3.268466
239.669347	3554.100191	17.068467	-0.046521	3.265022
239.396594	3546.134471	17.073472	-0.046465	3.261570
239.383892	3538.174409	17.078477	-0.046457	3.258127
239.437525	3530.146763	17.083482	-0.046462	3.254653
239.363969	3522.163132	17.088487	-0.046442	3.251191
239.343591	3514.173073	17.093491	-0.046433	3.247723
239.266742	3506.164449	17.098496	-0.046414	3.244242
239.295033	3498.236541	17.103501	-0.046414	3.240796
239.361709	3490.247535	17.108506	-0.046421	3.237322
239.294537	3482.228680	17.113511	-0.046403	3.233825
239.319337	3474.167757	17.118515	-0.046402	3.230310
239.026947	3466.198817	17.123520	-0.046342	3.226818
239.019080	3458.227011	17.128525	-0.046336	3.223333
239.007879	3450.234913	17.133530	-0.046328	3.219835
238.901727	3442.267554	17.138535	-0.046303	3.216341
238.967761	3434.289850	17.143539	-0.046310	3.212845
239.105056	3426.236610	17.148544	-0.046330	3.209314
239.056242	3418.287146	17.153549	-0.046316	3.205818
238.886706	3410.330162	17.158554	-0.046279	3.202310
238.901251	3402.347507	17.163559	-0.046277	3.198795
238.923265	3394.356640	17.168563	-0.046275	3.195272
238.806307	3386.340469	17.173568	-0.046248	3.191728
238.790340	3378.355387	17.178573	-0.046240	3.188198
238.794397	3370.337750	17.183578	-0.046235	3.184651
238.699056	3362.402685	17.188583	-0.046212	3.181132
238.706941	3354.429237	17.193587	-0.046209	3.177597
238.460204	3346.403428	17.198592	-0.046157	3.174023
238.541086	3338.405021	17.203597	-0.046167	3.170472
238.318146	3330.458937	17.208602	-0.046120	3.166927
238.421968	3322.448181	17.213607	-0.046134	3.163363
238.631288	3314.468352	17.218611	-0.046168	3.159814
238.462417	3306.515997	17.223616	-0.046131	3.156256
238.606656	3298.484936	17.228621	-0.046153	3.152673
238.415223	3290.481766	17.233626	-0.046112	3.149084
238.262284	3282.491018	17.238631	-0.046078	3.145498
238.278309	3274.556908	17.243635	-0.046076	3.141940
238.229692	3266.513732	17.248640	-0.046061	3.138327
238.343019	3258.556926	17.253645	-0.046077	3.134755
238.171970	3250.560905	17.258650	-0.046040	3.131149
238.118129	3242.572993	17.263655	-0.046024	3.127548
238.197457	3234.569369	17.268659	-0.046034	3.123941
238.102022	3226.624069	17.273664	-0.046011	3.120349
237.899495	3218.676526	17.278669	-0.045968	3.116747
237.750577	3210.652283	17.283674	-0.045935	3.113108
237.986084	3202.623247	17.288679	-0.045973	3.109481
238.016007	3194.655651	17.293683	-0.045974	3.105867
237.819247	3186.684984	17.298688	-0.045932	3.102238
237.845825	3178.699963	17.303693	-0.045931	3.098608
237.919926	3170.707861	17.308698	-0.045940	3.094973
237.872260	3162.707260	17.313703	-0.045925	3.091324
237.920981	3154.713242	17.318707	-0.045929	3.087678
237.970272	3146.721075	17.323712	-0.045933	3.084028
237.955840	3138.798687	17.328717	-0.045925	3.080404
237.841225	3130.816772	17.333722	-0.045898	3.076743
237.619742	3122.776350	17.338727	-0.045852	3.073046
237.507537	3114.757015	17.343731	-0.045826	3.069359
237.511202	3106.761342	17.348736	-0.045821	3.065684
237.643820	3098.794614	17.353741	-0.045840	3.062024
237.558353	3090.823122	17.358746	-0.045819	3.058348
237.436868	3082.842640	17.363751	-0.045791	3.054660
237.305010	3074.876978	17.368755	-0.045761	3.050975
237.202586	3066.877492	17.373760	-0.045737	3.047271
237.297695	3058.908503	17.378765	-0.045749	3.043586
237.291948	3050.922530	17.383770	-0.045743	3.039884
237.100175	3042.979013	17.388775	-0.045702	3.036188
237.206618	3034.960591	17.393779	-0.045717	3.032468
237.041200	3026.957433	17.398784	-0.045680	3.028736
237.042217	3018.992428	17.403789	-0.045675	3.025026
237.074333	3011.004516	17.408794	-0.045676	3.021302
237.108290	3003.022236	17.413799	-0.045677	3.017576
237.081697	2995.048802	17.418803	-0.045667	3.013847
236.918362	2987.026959	17.423808	-0.045631	3.010084
237.053459	2979.047753	17.428813	-0.045651	3.006351
236.807833	2971.101218	17.433818	-0.045600	3.002609
237.016134	2963.098211	17.438823	-0.045633	2.998859
236.921218	2955.139162	17.443827	-0.045610	2.995110
236.791176	2947.111058	17.448832	-0.045581	2.991322
236.900325	2939.128005	17.453837	-0.045596	2.987562
236.820079	2931.139408	17.458842	-0.045575	2.983785
236.704953	2923.168642	17.463847	-0.045549	2.980010
236.639207	2915.236377	17.468851	-0.045531	2.976251
236.857529	2907.184420	17.473856	-0.045566	2.972445
236.696393	2899.222740	17.478861	-0.045531	2.968658
236.600357	2891.239376	17.483866	-0.045508	2.964859
236.564833	2883.287984	17.488871	-0.045496	2.961073
236.619740	2875.330496	17.493875	-0.045501	2.957284
236.435336	2867.317440	17.498880	-0.045461	2.953452
236.520689	2859.291612	17.503885	-0.045472	2.949622
236.466841	2851.313410	17.508890	-0.045457	2.945803
236.304868	2843.366428	17.513895	-0.045421	2.941988
236.311674	2835.401747	17.518899	-0.045417	2.938169
236.227364	2827.413806	17.523904	-0.045396	2.934328
235.983150	2819.438230	17.528909	-0.045345	2.930480
235.942835	2811.463302	17.533914	-0.045332	2.926638
236.055108	2803.440757	17.538919	-0.045348	2.922776
236.289501	2795.475476	17.543923	-0.045386	2.918944
236.037648	2787.504216	17.548928	-0.045334	2.915077
236.238163	2779.412696	17.553933	-0.045366	2.911171
236.040449	2771.452408	17.558938	-0.045324	2.907302
236.109026	2763.474072	17.563943	-0.045331	2.903434
236.125790	2755.523619	17.568947	-0.045329	2.899571
235.893036	2747.589591	17.573952	-0.045281	2.895697
236.024761	2739.578484	17.578957	-0.045300	2.891801
235.690694	2731.622842	17.583962	-0.045232	2.887901
235.800708	2723.617190	17.588967	-0.045248	2.883995
235.855424	2715.676955	17.593971	-0.045252	2.880113
235.639216	2707.693606	17.598976	-0.045207	2.876190
235.543553	2699.716042	17.603981	-0.045184	2.872271
235.660054	2691.690704	17.608986	-0.045200	2.868335
235.535731	2683.720489	17.613991	-0.045172	2.864407
235.484358	2675.783466	17.618995	-0.045157	2.860494
235.405303	2667.791513	17.624000	-0.045137	2.856547
235.661852	2659.783503	17.629005	-0.045179	2.852606
235.495148	2651.803377	17.634010	-0.045143	2.848649
235.363251	2643.841193	17.639015	-0.045113	2.844698
235.263588	2635.921079	17.644019	-0.045089	2.840763
235.128865	2627.920510	17.649024	-0.045059	2.836781
235.317726	2619.902562	17.654029	-0.045089	2.832804
235.330360	2611.904596	17.659034	-0.045086	2.828820
235.145956	2603.921634	17.664039	-0.045046	2.824828
235.058976	2595.985752	17.669043	-0.045024	2.820858
235.097658	2587.993050	17.674048	-0.045026	2.816862
235.210852	2580.006851	17.679053	-0.045042	2.812868
235.058163	2572.019601	17.684058	-0.045008	2.808852
234.936321	2564.029126	17.689063	-0.044980	2.804831
234.865091	2556.114408	17.694067	-0.044962	2.800844
234.768962	2548.142666	17.699072	-0.044939	2.796822
235.033410	2540.123385	17.704077	-0.044983	2.792792
234.808602	2532.134610	17.709082	-0.044935	2.788742
234.662285	2524.168175	17.714087	-0.044903	2.784702
234.770833	2516.221896	17.719091	-0.044918	2.780681
234.636989	2508.239685	17.724096	-0.044887	2.776622
234.707071	2500.242960	17.729101	-0.044895	2.772562
234.546998	2492.269497	17.734106	-0.044860	2.768494
234.553238	2484.271839	17.739111	-0.044856	2.764418
234.669848	2476.342693	17.744115	-0.044872	2.760377
234.545997	2468.364865	17.749120	-0.044844	2.756291
234.506375	2460.318951	17.754125	-0.044831	2.752169
234.694956	2452.276460	17.759130	-0.044861	2.748056
234.567986	2444.328725	17.764135	-0.044832	2.743967
234.424987	2436.417247	17.769139	-0.044800	2.739889
234.247694	2428.468389	17.774144	-0.044762	2.735784
234.245467	2420.464825	17.779149	-0.044756	2.731656
234.241784	2412.457835	17.784154	-0.044750	2.727519
234.087326	2404.504457	17.789159	-0.044716	2.723394
234.267857	2396.546146	17.794163	-0.044744	2.719281
234.029131	2388.604162	17.799168	-0.044695	2.715144
234.106116	2380.581432	17.804173	-0.044704	2.710979
234.281414	2372.598757	17.809178	-0.044731	2.706834
234.200321	2364.635044	17.814183	-0.044711	2.702677
234.005274	2356.706288	17.819187	-0.044669	2.698524
233.906281	2348.722211	17.824192	-0.044645	2.694342
234.103774	2340.715427	17.829197	-0.044677	2.690161
233.999631	2332.743139	17.834202	-0.044652	2.685972
233.907744	2324.802048	17.839207	-0.044630	2.681793
233.844630	2316.858635	17.844211	-0.044613	2.677609
233.587218	2308.858927	17.849216	-0.044559	2.673376
233.883791	2300.823015	17.854221	-0.044609	2.669152
233.740252	2292.856179	17.859226	-0.044577	2.664930
233.682577	2284.901004	17.864231	-0.044561	2.660713
233.568155	2276.983631	17.869235	-0.044535	2.656506
233.499540	2268.972859	17.874240	-0.044516	2.652246
233.606337	2260.995419	17.879245	-0.044531	2.648007
233.439748	2253.019752	17.884250	-0.044495	2.643745
233.269737	2245.063890	17.889255	-0.044458	2.639487
233.600423	2237.094624	17.894259	-0.044514	2.635247
233.465256	2229.101067	17.899264	-0.044484	2.630957
233.346444	2221.157855	17.904269	-0.044456	2.626688
233.152904	2213.180553	17.909274	-0.044415	2.622388
233.258554	2205.201409	17.914279	-0.044429	2.618100
233.318159	2197.249084	17.919283	-0.044435	2.613817
233.062745	2189.247226	17.924288	-0.044382	2.609479
233.181571	2181.298469	17.929293	-0.044399	2.605188
233.109015	2173.335922	17.934298	-0.044380	2.600869
233.013461	2165.394685	17.939303	-0.044357	2.596552
233.115536	2157.291652	17.944307	-0.044371	2.592154
232.880983	2149.265366	17.949312	-0.044322	2.587768
232.838882	2141.336491	17.954317	-0.044308	2.583440
232.945918	2133.395625	17.959322	-0.044323	2.579109
232.789534	2125.438756	17.964327	-0.044289	2.574743
232.725094	2117.492423	17.969331	-0.044271	2.570383
232.547862	2109.541179	17.974336	-0.044233	2.566004
232.849981	2101.560046	17.979341	-0.044284	2.561634
232.664971	2093.622861	17.984346	-0.044244	2.557248
232.573784	2085.653885	17.989351	-0.044222	2.552843
232.542385	2077.684074	17.994355	-0.044211	2.548434
232.577666	2069.690025	17.999360	-0.044212	2.544008
232.641460	2061.738555	18.004365	-0.044219	2.539601
232.473182	2053.803783	18.009370	-0.044182	2.535178
232.412657	2045.817091	18.014375	-0.044166	2.530727
232.420393	2037.856164	18.019379	-0.044162	2.526287
232.325106	2029.883342	18.024384	-0.044139	2.521825
232.330587	2021.952992	18.029389	-0.044134	2.517387
232.340310	2013.978224	18.034394	-0.044131	2.512915
232.204989	2005.968837	18.039399	-0.044100	2.508406
232.358786	1998.006508	18.044403	-0.044124	2.503936
232.316562	1990.045419	18.049408	-0.044110	2.499445
232.242247	1982.091210	18.054413	-0.044091	2.494947
232.037865	1974.135145	18.059418	-0.044048	2.490431
232.013064	1966.166225	18.064423	-0.044038	2.485912
231.962489	1958.233277	18.069427	-0.044023	2.481403
231.752731	1950.271047	18.074432	-0.043979	2.476858
231.886614	1942.302069	18.079437	-0.043999	2.472326
231.978501	1934.303107	18.084442	-0.044010	2.467765
231.790292	1926.359266	18.089447	-0.043970	2.463207
231.974985	1918.402148	18.094451	-0.043999	2.458660
231.667635	1910.455631	18.099456	-0.043937	2.454074
231.672366	1902.470203	18.104461	-0.043932	2.449481
231.474502	1894.530418	18.109466	-0.043890	2.444890
231.771476	1886.551905	18.114471	-0.043940	2.440305
231.712700	1878.626975	18.119475	-0.043924	2.435716
231.554049	1870.591353	18.124480	-0.043889	2.431046
231.563961	1862.607532	18.129485	-0.043886	2.426411
231.448385	1854.675664	18.134490	-0.043859	2.421787
231.406244	1846.724399	18.139495	-0.043846	2.417148
231.222726	1838.791425	18.144499	-0.043806	2.412500
231.252743	1830.793236	18.149504	-0.043806	2.407822
231.187402	1822.850120	18.154509	-0.043789	2.403159
231.033171	1814.936690	18.159514	-0.043755	2.398498
231.130050	1806.937391	18.164519	-0.043768	2.393797
231.210009	1798.978208	18.169523	-0.043777	2.389109
230.878693	1791.030269	18.174528	-0.043710	2.384386
231.055721	1783.062264	18.179533	-0.043738	2.379682
231.012286	1775.121616	18.184538	-0.043725	2.374967
230.613392	1767.188410	18.189543	-0.043645	2.370219
230.716238	1759.220813	18.194547	-0.043659	2.365481
230.627942	1751.256731	18.199552	-0.043637	2.360721
230.723882	1743.312567	18.204557	-0.043650	2.355977
230.631504	1735.335634	18.209562	-0.043627	2.351189
230.501005	1727.370814	18.214567	-0.043598	2.346395
230.650412	1719.397608	18.219571	-0.043620	2.341609
230.526129	1711.464569	18.224576	-0.043592	2.336816
230.574156	1703.500446	18.229581	-0.043595	2.332008
230.601284	1695.523102	18.234586	-0.043595	2.327180
230.430056	1687.600384	18.239591	-0.043558	2.322359
230.547019	1679.652557	18.244595	-0.043574	2.317536
230.459936	1671.705066	18.249600	-0.043553	2.312687
230.485137	1663.728011	18.254605	-0.043552	2.307818
230.180425	1655.817592	18.259610	-0.043490	2.302953
230.120615	1647.862220	18.264615	-0.043474	2.298070
230.276567	1639.894114	18.269619	-0.043498	2.293187
230.007165	1631.959148	18.274624	-0.043442	2.288278
230.055738	1624.003593	18.279629	-0.043446	2.283373
230.021272	1616.075547	18.284634	-0.043434	2.278467
229.965188	1608.096121	18.289639	-0.043418	2.273517
229.883042	1600.092519	18.294643	-0.043398	2.268539
229.743612	1592.153301	18.299648	-0.043367	2.263585
229.854439	1584.199542	18.304653	-0.043382	2.258633
229.812275	1576.255233	18.309658	-0.043369	2.253662
229.609555	1568.310511	18.314663	-0.043326	2.248667
229.860269	1560.345421	18.319667	-0.043367	2.243686
229.821959	1552.407465	18.324672	-0.043355	2.238687
229.782836	1544.484896	18.329677	-0.043342	2.233686
229.693264	1536.529927	18.334682	-0.043320	2.228649
229.663502	1528.578700	18.339687	-0.043309	2.223608
229.736647	1520.635236	18.344691	-0.043318	2.218570
229.658957	1512.694703	18.349696	-0.043298	2.213508
229.513085	1504.761930	18.354701	-0.043265	2.208434
229.389123	1496.826833	18.359706	-0.043237	2.203349
229.205860	1488.907309	18.364711	-0.043198	2.198256
229.332103	1480.950365	18.369715	-0.043216	2.193156
229.160342	1472.970473	18.374720	-0.043179	2.188001
229.170669	1465.025230	18.379725	-0.043175	2.182874
229.267888	1457.078345	18.384730	-0.043188	2.177741
229.327430	1449.121565	18.389735	-0.043194	2.172587
229.232480	1441.198640	18.394739	-0.043171	2.167428
229.150504	1433.255215	18.399744	-0.043150	2.162244
229.169414	1425.335103	18.404749	-0.043149	2.157073
229.023727	1417.405800	18.409754	-0.043116	2.151867
228.981595	1409.444609	18.414759	-0.043103	2.146638
229.139713	1401.497598	18.419763	-0.043127	2.141424
228.748074	1393.609913	18.424768	-0.043049	2.136185
228.745915	1385.654298	18.429773	-0.043043	2.130925
228.723482	1377.712523	18.434778	-0.043034	2.125659
228.598951	1369.786596	18.439783	-0.043005	2.120380
228.634243	1361.864447	18.444787	-0.043007	2.115107
228.456446	1353.850141	18.449792	-0.042968	2.109738
228.553966	1345.888488	18.454797	-0.042981	2.104417
228.594389	1337.959793	18.459802	-0.042983	2.099099
228.410207	1330.063087	18.464807	-0.042944	2.093767
228.608246	1322.095064	18.469811	-0.042975	2.088411
228.624267	1314.166169	18.474816	-0.042973	2.083050
228.512463	1306.267984	18.479821	-0.042947	2.077684
228.506860	1298.338099	18.484826	-0.042941	2.072292
228.361508	1290.410351	18.489831	-0.042908	2.066874
228.553506	1282.454175	18.494835	-0.042939	2.061455
228.315261	1274.561918	18.499840	-0.042889	2.056024
228.182444	1266.638016	18.504845	-0.042859	2.050566
228.331947	1258.682322	18.509850	-0.042882	2.045101
228.061600	1250.792740	18.514855	-0.042826	2.039624
228.086959	1242.875406	18.519859	-0.042826	2.034143
228.134799	1234.882450	18.524864	-0.042829	2.028597
228.154362	1226.955754	18.529869	-0.042828	2.023079
228.029683	1219.056989	18.534874	-0.042799	2.017551
228.179161	1211.089758	18.539879	-0.042822	2.011988
227.985727	1203.205405	18.544883	-0.042780	2.006432
227.677354	1195.311794	18.549888	-0.042718	2.000842
227.835049	1187.373481	18.554893	-0.042742	1.995254
227.781282	1179.446858	18.559898	-0.042726	1.989636
227.765549	1171.503171	18.564903	-0.042718	1.983994
227.905706	1163.586635	18.569907	-0.042739	1.978371
227.750117	1155.679403	18.574912	-0.042705	1.972708
227.666215	1147.754880	18.579917	-0.042684	1.967024
227.705087	1139.842750	18.584922	-0.042686	1.961345
227.428829	1131.954153	18.589927	-0.042629	1.955633
227.535148	1123.982228	18.594931	-0.042644	1.949885
227.179914	1116.086440	18.599936	-0.042572	1.944126
227.464145	1108.126097	18.604941	-0.042620	1.938372
227.481228	1100.219296	18.609946	-0.042618	1.932610
227.145144	1092.323600	18.614951	-0.042550	1.926801
227.112284	1084.434255	18.619955	-0.042539	1.921012
227.160919	1076.494915	18.624960	-0.042542	1.915178
226.907764	1068.610995	18.629965	-0.042490	1.909333
226.972048	1060.684135	18.634970	-0.042497	1.903474
227.028330	1052.764119	18.639975	-0.042502	1.897602
226.934625	1044.878345	18.644979	-0.042479	1.891719
226.971141	1036.935994	18.649984	-0.042481	1.885791
227.044387	1029.023150	18.654989	-0.042489	1.879870
227.017311	1021.139237	18.659994	-0.042479	1.873941
226.666485	1013.241638	18.664999	-0.042408	1.867945
226.586067	1005.346874	18.670003	-0.042388	1.861964
226.632219	997.424670	18.675008	-0.042391	1.855957
226.546703	989.511982	18.680013	-0.042370	1.849922
226.404864	981.635831	18.685018	-0.042338	1.843889
226.347606	973.737374	18.690023	-0.042323	1.837829
226.556215	965.814563	18.695027	-0.042356	1.831761
226.272263	957.931008	18.700032	-0.042298	1.825645
226.414211	950.011839	18.705037	-0.042319	1.819532
226.221158	942.157189	18.710042	-0.042278	1.813408
226.116006	934.229633	18.715047	-0.042253	1.807217
226.150598	926.354099	18.720051	-0.042254	1.801063
225.961165	918.486702	18.725056	-0.042214	1.794866
226.164613	910.492838	18.730061	-0.042246	1.788596
226.058364	902.620626	18.735066	-0.042221	1.782363
226.118425	894.725185	18.740071	-0.042227	1.776110
226.069571	886.835636	18.745075	-0.042213	1.769825
225.896036	878.965839	18.750080	-0.042175	1.763519
226.022950	871.079354	18.755085	-0.042194	1.757214
225.887205	863.209751	18.760090	-0.042163	1.750867
225.575271	855.353098	18.765095	-0.042100	1.744485
225.528494	847.487941	18.770099	-0.042086	1.738106
225.536797	839.582084	18.775104	-0.042082	1.731678
225.445644	831.700528	18.780109	-0.042060	1.725233
225.345141	823.855826	18.785114	-0.042036	1.718792
225.254522	815.964183	18.790119	-0.042014	1.712290
225.244940	808.067130	18.795123	-0.042007	1.705769
225.170754	800.195947	18.800128	-0.041988	1.699237
225.081289	792.329935	18.805133	-0.041966	1.692681
225.037892	784.445728	18.810138	-0.041953	1.686091
224.944599	776.588157	18.815143	-0.041930	1.679490
224.872908	768.737911	18.820147	-0.041911	1.672872
225.095594	760.808960	18.825152	-0.041948	1.666201
225.000684	752.967832	18.830157	-0.041925	1.659536
224.901219	745.122395	18.835162	-0.041901	1.652838
224.810507	737.249669	18.840167	-0.041879	1.646092
224.799272	729.413258	18.845171	-0.041872	1.639359
224.711202	721.541781	18.850176	-0.041850	1.632558
224.582484	713.648115	18.855181	-0.041821	1.625704
224.657930	705.784319	18.860186	-0.041830	1.618875
224.416741	697.954724	18.865191	-0.041779	1.612003
224.446548	690.091601	18.870195	-0.041780	1.605110
224.389233	682.265363	18.875200	-0.041764	1.598207
224.317636	674.414310	18.880205	-0.041745	1.591251
224.237271	666.579549	18.885210	-0.041725	1.584277
224.142111	658.735094	18.890215	-0.041702	1.577261
224.474270	650.838874	18.895219	-0.041759	1.570230
224.170793	643.043464	18.900224	-0.041697	1.563165
224.081674	635.228385	18.905229	-0.041675	1.556081
224.246689	627.350509	18.910234	-0.041701	1.548946
223.949750	619.551002	18.915239	-0.041640	1.541781
224.010168	611.710630	18.920243	-0.041646	1.534598
223.701281	603.904153	18.925248	-0.041584	1.527356
223.715598	596.068913	18.930253	-0.041581	1.520103
223.836065	588.239110	18.935258	-0.041598	1.512836
223.782596	580.399454	18.940263	-0.041583	1.505498
223.579277	572.629753	18.945267	-0.041540	1.498167
223.482533	564.803785	18.950272	-0.041517	1.490763
223.521410	556.976464	18.955277	-0.041519	1.483342
223.548976	549.176798	18.960282	-0.041519	1.475908
223.482939	541.309166	18.965287	-0.041501	1.468356
223.429240	533.512926	18.970291	-0.041486	1.460837
223.335553	525.726547	18.975296	-0.041463	1.453281
223.302189	517.910124	18.980301	-0.041452	1.445667
223.113084	510.166369	18.985306	-0.041412	1.438058
222.914950	502.382138	18.990311	-0.041370	1.430367
223.028917	494.568051	18.995315	-0.041386	1.422656
222.857240	486.803862	19.000320	-0.041348	1.414906
222.685439	479.026142	19.005325	-0.041311	1.407100
222.875031	471.226212	19.010330	-0.041341	1.399287
222.663700	463.458882	19.015335	-0.041297	1.391397
222.608068	455.683421	19.020339	-0.041281	1.383480
222.726444	447.885888	19.025344	-0.041298	1.375524
222.609009	440.121914	19.030349	-0.041271	1.367516
222.497699	432.385575	19.035354	-0.041245	1.359490
222.286576	424.644914	19.040359	-0.041201	1.351395
222.563273	416.838675	19.045363	-0.041247	1.343267
222.374354	409.120325	19.050368	-0.041207	1.335101
222.129682	401.395165	19.055373	-0.041156	1.326868
222.185561	393.650118	19.060378	-0.041161	1.318615
221.984681	385.842262	19.065383	-0.041119	1.310197
222.001616	378.063676	19.070387	-0.041117	1.301795
221.949665	370.344556	19.075392	-0.041102	1.293391
221.960369	362.609461	19.080397	-0.041099	1.284926
221.859776	354.929156	19.085402	-0.041075	1.276444
221.547711	347.244533	19.090407	-0.041012	1.267862
221.626974	339.525232	19.095411	-0.041021	1.259256
221.560046	331.818515	19.100416	-0.041004	1.250577
221.391702	324.149549	19.105421	-0.040967	1.241861
221.510122	316.436851	19.110426	-0.040984	1.233088
221.320181	308.752222	19.115431	-0.040944	1.224225
221.455568	301.053158	19.120435	-0.040964	1.215345
221.154462	293.411298	19.125440	-0.040903	1.206379
221.060639	285.761236	19.130445	-0.040880	1.197378
221.087219	278.090142	19.135450	-0.040880	1.188308
220.800908	270.465046	19.140455	-0.040821	1.179160
221.106283	262.762602	19.145459	-0.040873	1.169968
221.038586	255.133119	19.150464	-0.040855	1.160715
220.850313	247.514612	19.155469	-0.040815	1.151376
220.692466	239.881911	19.160474	-0.040781	1.141949
220.631830	232.263758	19.165479	-0.040765	1.132482
220.410824	224.682021	19.170483	-0.040718	1.122947
220.378247	217.078656	19.175488	-0.040707	1.113344
220.280710	209.482986	19.180493	-0.040684	1.103652
220.316586	201.895542	19.185498	-0.040686	1.093915
220.101259	194.334232	19.190503	-0.040640	1.084068
220.065561	186.776668	19.195507	-0.040629	1.074177
220.145868	179.182125	19.200512	-0.040639	1.064171
219.995939	171.656186	19.205517	-0.040606	1.054108
219.887254	164.120722	19.210522	-0.040580	1.043945
219.777355	156.621196	19.215527	-0.040555	1.033732
219.750120	149.104658	19.220531	-0.040545	1.023412
219.512366	141.637253	19.225536	-0.040496	1.013005
219.511052	134.132442	19.230541	-0.040490	1.002494
219.573145	126.633270	19.235546	-0.040497	0.991897
219.247377	119.184826	19.240551	-0.040431	0.981160
219.217535	111.735441	19.245555	-0.040421	0.970378
219.173643	104.295971	19.250560	-0.040408	0.959486
219.050097	96.885844	19.255565	-0.040380	0.948492
219.004539	89.488306	19.260570	-0.040366	0.937408
218.540362	82.156601	19.265575	-0.040275	0.926180
218.488108	74.789500	19.270579	-0.040260	0.914871
218.002948	67.491145	19.275584	-0.040165	0.903409
217.679631	60.420378	19.280589	-0.040100	0.892205