Fri Mar 12 13:04:08 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.437078	-0.046256	0.000000	-0.000044	0.719600

0.558866	-0.063203	0.005005	-0.000067	0.719609
0.292763	-0.018987	0.010010	-0.000017	0.719603
0.501275	-0.056050	0.015014	-0.000056	0.719603
0.504099	-0.053275	0.020019	-0.000056	0.719609
0.424284	-0.044809	0.025024	-0.000041	0.719598
0.297586	-0.017660	0.030029	-0.000018	0.719607
0.397794	-0.036821	0.035034	-0.000036	0.719604
0.485369	-0.052465	0.040038	-0.000052	0.719604
0.404337	-0.033489	0.045043	-0.000037	0.719612
0.419847	-0.127782	0.050048	-0.000040	0.719432
0.435260	-0.208501	0.055053	-0.000043	0.719278
0.282952	-0.183520	0.060058	-0.000014	0.719274
0.499133	-0.223097	0.065062	-0.000054	0.719271
0.518492	-0.223347	0.070067	-0.000058	0.719277
0.565972	-0.236679	0.075072	-0.000067	0.719268
0.488151	-0.218157	0.080077	-0.000052	0.719277
0.332456	-0.193088	0.085082	-0.000023	0.719271
0.372929	-0.345188	0.090086	-0.000030	0.718985
0.385077	-0.354836	0.095091	-0.000033	0.718971
0.474687	-0.376380	0.100096	-0.000049	0.718959
0.415842	-0.361240	0.105101	-0.000038	0.718968
0.278044	-0.337181	0.110106	-0.000013	0.718967
0.280603	-0.399859	0.115110	-0.000013	0.718844
0.535199	-0.543003	0.120115	-0.000060	0.718651
0.398462	-0.524390	0.125120	-0.000035	0.718640
0.378299	-0.514599	0.130125	-0.000031	0.718652
0.312197	-0.505957	0.135130	-0.000018	0.718646
0.336979	-0.641739	0.140134	-0.000023	0.718386
0.455790	-0.675673	0.145139	-0.000045	0.718361
0.168965	-0.628666	0.150144	0.000009	0.718352
0.416418	-0.669585	0.155149	-0.000037	0.718359
0.223231	-0.798096	0.160154	-0.000001	0.718037
0.367334	-0.832264	0.165158	-0.000028	0.718020
0.618681	-0.875065	0.170163	-0.000075	0.718023
0.561284	-0.947797	0.175168	-0.000064	0.717859
0.307517	-0.979256	0.180173	-0.000017	0.717708
0.497687	-1.014360	0.185178	-0.000052	0.717705
0.541960	-1.081794	0.190182	-0.000060	0.717587
0.352090	-1.148641	0.195187	-0.000024	0.717388
0.340296	-1.149863	0.200192	-0.000022	0.717381
0.491790	-1.234198	0.205197	-0.000050	0.717268
0.316403	-1.292217	0.210202	-0.000018	0.717091
0.337834	-1.297936	0.215206	-0.000021	0.717087
0.273464	-1.387026	0.220211	-0.000009	0.716888
0.054467	-1.415225	0.225216	0.000032	0.716755
-0.039698	-1.395896	0.230221	0.000049	0.716760
0.124601	-1.563714	0.235226	0.000019	0.716485
0.181919	-1.592260	0.240230	0.000008	0.716449
0.083209	-1.621706	0.245235	0.000027	0.716356
-0.029083	-1.715039	0.250240	0.000048	0.716131
0.211365	-1.753900	0.255245	0.000003	0.716139
-0.044516	-1.817603	0.260250	0.000051	0.715922
-0.020930	-1.840993	0.265254	0.000046	0.715884
0.079587	-1.939087	0.270259	0.000028	0.715725
-0.071999	-2.003630	0.275264	0.000056	0.715543
-0.096401	-2.028144	0.280269	0.000061	0.715486
-0.191344	-2.138989	0.285274	0.000079	0.715232
-0.279705	-2.123728	0.290278	0.000095	0.715231
-0.130013	-2.303321	0.295283	0.000068	0.714928
-0.265284	-2.291108	0.300288	0.000093	0.714904
-0.305425	-2.401742	0.305293	0.000100	0.714670
-0.407357	-2.414060	0.310298	0.000119	0.714609
-0.525478	-2.507765	0.315302	0.000142	0.714381
-0.864594	-2.495773	0.320307	0.000205	0.714285
-3.082307	-2.155370	0.325312	0.000618	0.714176
-3.236675	-2.228753	0.330317	0.000646	0.713976
-2.656090	-2.334320	0.335322	0.000538	0.713971
-3.489209	-2.244453	0.340326	0.000694	0.713855
-4.136903	-2.227658	0.345331	0.000814	0.713659
-3.973076	-2.262507	0.350336	0.000784	0.713647
-4.330348	-2.194228	0.355341	0.000850	0.713656
-4.749020	-2.260473	0.360346	0.000929	0.713376
-4.981398	-2.226847	0.365350	0.000972	0.713361
-5.150309	-2.192718	0.370355	0.001003	0.713368
-5.117315	-2.239295	0.375360	0.000997	0.713287
-5.985449	-2.214673	0.380365	0.001159	0.713028
-5.710896	-2.265128	0.385370	0.001108	0.713025
-6.128772	-2.192994	0.390374	0.001186	0.713021
-5.972314	-2.215622	0.395379	0.001157	0.713031
-6.544113	-2.275113	0.400384	0.001263	0.712709
-6.898443	-2.209006	0.405389	0.001329	0.712715
-7.103539	-2.175253	0.410394	0.001368	0.712710
-6.904757	-2.211933	0.415398	0.001331	0.712707
-6.652697	-2.301346	0.420403	0.001284	0.712618
-8.185141	-2.146191	0.425408	0.001569	0.712383
-7.841777	-2.203618	0.430413	0.001505	0.712391
-7.772913	-2.215856	0.435418	0.001493	0.712390
-7.952576	-2.186005	0.440422	0.001526	0.712386
-7.674304	-2.242061	0.445427	0.001474	0.712373
-8.440990	-2.249627	0.450432	0.001617	0.712086
-8.471986	-2.239842	0.455437	0.001623	0.712094
-8.848815	-2.174387	0.460442	0.001693	0.712090
-8.970409	-2.154334	0.465446	0.001716	0.712087
-8.427730	-2.246456	0.470451	0.001615	0.712096
-8.910386	-2.253513	0.475456	0.001705	0.711910
-9.979899	-2.134792	0.480461	0.001904	0.711767
-9.309277	-2.255315	0.485466	0.001779	0.711765
-9.784264	-2.173228	0.490470	0.001868	0.711760
-9.883467	-2.150469	0.495475	0.001886	0.711770
-9.523635	-2.219605	0.500480	0.001820	0.711760
-9.731185	-2.249372	0.505485	0.001858	0.711626
-10.815567	-2.140333	0.510490	0.002060	0.711458
-10.357955	-2.223919	0.515494	0.001975	0.711454
-10.100876	-2.265196	0.520499	0.001927	0.711463
-10.805992	-2.143899	0.525504	0.002059	0.711454
-10.773285	-2.146917	0.530509	0.002053	0.711460
-10.470704	-2.211173	0.535514	0.001996	0.711439
-11.465697	-2.186570	0.540518	0.002182	0.711134
-11.500703	-2.175410	0.545523	0.002188	0.711144
-11.776654	-2.130194	0.550528	0.002240	0.711136
-11.297069	-2.212493	0.555533	0.002151	0.711142
-11.479958	-2.179949	0.560538	0.002185	0.711142
-11.875128	-2.112940	0.565542	0.002258	0.711135
-11.310145	-2.236897	0.570547	0.002153	0.711088
-12.187781	-2.189494	0.575552	0.002317	0.710870
-12.128485	-2.197330	0.580557	0.002306	0.710876
-12.100505	-2.204513	0.585562	0.002301	0.710871
-12.293738	-2.170515	0.590566	0.002337	0.710870
-12.347198	-2.158141	0.595571	0.002347	0.710876
-12.009985	-2.221094	0.600576	0.002284	0.710870
-12.479711	-2.281598	0.605581	0.002372	0.710582
-13.151082	-2.185997	0.610586	0.002497	0.710534
-13.222792	-2.174045	0.615590	0.002510	0.710532
-12.587886	-2.281842	0.620595	0.002392	0.710542
-13.221862	-2.174186	0.625600	0.002510	0.710532
-13.552802	-2.112364	0.630605	0.002572	0.710537
-12.919415	-2.273035	0.635610	0.002454	0.710442
-14.120127	-2.171500	0.640614	0.002678	0.710217
-14.030901	-2.182955	0.645619	0.002661	0.710225
-14.249587	-2.148364	0.650624	0.002702	0.710217
-14.102761	-2.171685	0.655629	0.002675	0.710222
-13.934036	-2.203479	0.660634	0.002643	0.710219
-14.465813	-2.109460	0.665638	0.002742	0.710217
-13.823086	-2.267518	0.670643	0.002623	0.710130
-14.937632	-2.188584	0.675648	0.002830	0.709890
-15.216504	-2.136393	0.680653	0.002882	0.709895
-15.155568	-2.146947	0.685658	0.002871	0.709896
-14.847063	-2.203924	0.690662	0.002814	0.709892
-15.094792	-2.155644	0.695667	0.002860	0.709900
-15.217958	-2.138073	0.700672	0.002883	0.709891
-14.881951	-2.202373	0.705677	0.002820	0.709882
-15.417502	-2.247573	0.710682	0.002920	0.709600
-15.985208	-2.149565	0.715686	0.003026	0.709594
-15.981084	-2.145975	0.720691	0.003025	0.709602
-15.671072	-2.206461	0.725696	0.002968	0.709592
-16.026869	-2.139741	0.730701	0.003034	0.709598
-15.643714	-2.207994	0.735706	0.002963	0.709598
-15.599783	-2.257037	0.740710	0.002955	0.709516
-16.702104	-2.181881	0.745715	0.003160	0.709273
-16.720756	-2.183946	0.750720	0.003163	0.709262
-16.737568	-2.178265	0.755725	0.003167	0.709267
-16.442908	-2.231332	0.760730	0.003112	0.709266
-16.880723	-2.155886	0.765734	0.003193	0.709261
-16.595571	-2.200237	0.770739	0.003140	0.709273
-16.509054	-2.275766	0.775744	0.003124	0.709153
-17.593880	-2.178473	0.780749	0.003326	0.708961
-17.407763	-2.211299	0.785754	0.003292	0.708961
-17.737427	-2.155515	0.790758	0.003353	0.708955
-17.544400	-2.185518	0.795763	0.003317	0.708964
-17.617574	-2.176226	0.800768	0.003331	0.708956
-17.623358	-2.173876	0.805773	0.003332	0.708959
-17.605674	-2.240033	0.810778	0.003329	0.708832
-19.075718	-2.074110	0.815782	0.003603	0.708640
-18.291659	-2.208987	0.820787	0.003457	0.708649
-18.447289	-2.186673	0.825792	0.003486	0.708638
-18.821090	-2.117057	0.830797	0.003556	0.708644
-18.423124	-2.188109	0.835802	0.003482	0.708644
-18.232200	-2.225262	0.840806	0.003446	0.708637
-18.239426	-2.265636	0.845811	0.003448	0.708554
-19.508627	-2.139088	0.850816	0.003684	0.708354
-19.049114	-2.219320	0.855821	0.003599	0.708357
-19.103757	-2.208847	0.860826	0.003609	0.708359
-19.682408	-2.109653	0.865830	0.003717	0.708350
-19.386076	-2.157101	0.870835	0.003661	0.708361
-19.258799	-2.186375	0.875840	0.003638	0.708348
-19.425004	-2.213274	0.880845	0.003669	0.708234
-20.504506	-2.127064	0.885850	0.003870	0.708021
-20.144555	-2.195549	0.890854	0.003803	0.708013
-20.066914	-2.206201	0.895859	0.003789	0.708019
-20.500423	-2.130576	0.900864	0.003869	0.708015
-20.464625	-2.134276	0.905869	0.003863	0.708021
-20.271634	-2.168136	0.910874	0.003827	0.708021
-20.636377	-2.107764	0.915878	0.003895	0.708012
-20.772395	-2.213500	0.920883	0.003920	0.707751
-21.414209	-2.125884	0.925888	0.004040	0.707697
-21.578931	-2.095674	0.930893	0.004071	0.707699
-21.413579	-2.121806	0.935898	0.004040	0.707706
-21.411161	-2.123956	0.940902	0.004040	0.707702
-21.089141	-2.176845	0.945907	0.003980	0.707711
-21.464977	-2.113560	0.950912	0.004050	0.707703
-21.464967	-2.146839	0.955917	0.004050	0.707636
-22.046777	-2.170825	0.960922	0.004158	0.707380
-21.992949	-2.182643	0.965926	0.004148	0.707375
-22.252379	-2.132362	0.970931	0.004197	0.707383
-22.157787	-2.152535	0.975936	0.004179	0.707377
-21.746149	-2.224319	0.980941	0.004103	0.707380
-22.201183	-2.141351	0.985946	0.004187	0.707383
-22.240124	-2.176462	0.990950	0.004195	0.707299
-22.839185	-2.174096	0.995955	0.004306	0.707089
-22.959910	-2.155228	1.000960	0.004329	0.707084
-23.268181	-2.098186	1.005965	0.004386	0.707088
-22.746352	-2.190818	1.010970	0.004289	0.707088
-22.948963	-2.159647	1.015974	0.004327	0.707078
-23.196721	-2.112653	1.020979	0.004373	0.707084
-22.981489	-2.178706	1.025984	0.004333	0.707028
-23.650907	-2.194768	1.030989	0.004458	0.706756
-23.774817	-2.173270	1.035994	0.004481	0.706755
-24.108196	-2.116376	1.040998	0.004543	0.706749
-23.409455	-2.236310	1.046003	0.004413	0.706759
-23.837592	-2.163731	1.051008	0.004493	0.706751
-24.209702	-2.095504	1.056013	0.004562	0.706755
-23.725472	-2.225230	1.061018	0.004472	0.706667
-24.819586	-2.141742	1.066022	0.004676	0.706443
-24.811773	-2.138441	1.071027	0.004675	0.706452
-24.970988	-2.113640	1.076032	0.004704	0.706445
-24.584044	-2.181728	1.081037	0.004632	0.706447
-24.390418	-2.213569	1.086042	0.004597	0.706452
-24.915127	-2.123810	1.091046	0.004694	0.706444
-24.418550	-2.262982	1.096051	0.004602	0.706342
-25.553228	-2.167585	1.101056	0.004813	0.706127
-25.468134	-2.180121	1.106061	0.004797	0.706132
-25.471572	-2.178116	1.111066	0.004798	0.706135
-25.655868	-2.150278	1.116070	0.004833	0.706125
-25.309551	-2.205729	1.121075	0.004768	0.706137
-25.353767	-2.200843	1.126080	0.004776	0.706131
-25.719283	-2.233090	1.131085	0.004845	0.705935
-26.434978	-2.138737	1.136090	0.004978	0.705868
-26.539957	-2.124454	1.141094	0.004998	0.705859
-25.971483	-2.219589	1.146099	0.004892	0.705871
-26.316309	-2.163132	1.151104	0.004956	0.705861
-26.469347	-2.134498	1.156109	0.004985	0.705864
-25.928287	-2.249002	1.161114	0.004884	0.705827
-26.899203	-2.227476	1.166118	0.005065	0.705522
-26.839001	-2.233986	1.171123	0.005054	0.705531
-27.182136	-2.177050	1.176128	0.005118	0.705522
-27.079537	-2.192476	1.181133	0.005099	0.705528
-27.244321	-2.161555	1.186138	0.005129	0.705531
-27.408548	-2.135078	1.191142	0.005160	0.705525
-27.026982	-2.278931	1.196147	0.005089	0.705372
-28.299972	-2.131687	1.201152	0.005326	0.705212
-28.164824	-2.154158	1.206157	0.005301	0.705215
-27.697062	-2.235420	1.211162	0.005214	0.705219
-28.051835	-2.177453	1.216166	0.005280	0.705208
-28.056076	-2.172400	1.221171	0.005281	0.705217
-27.979051	-2.189472	1.226176	0.005267	0.705210
-28.142040	-2.274586	1.231181	0.005297	0.704980
-28.822472	-2.196889	1.236186	0.005424	0.704892
-29.222399	-2.127613	1.241190	0.005498	0.704887
-28.799166	-2.200785	1.246195	0.005420	0.704892
-29.143046	-2.139602	1.251200	0.005484	0.704892
-29.369070	-2.099585	1.256205	0.005526	0.704891
-28.923608	-2.177339	1.261210	0.005443	0.704894
-29.143028	-2.220376	1.266214	0.005484	0.704728
-30.164200	-2.104924	1.271219	0.005674	0.704594
-29.794764	-2.175828	1.276224	0.005606	0.704584
-29.991575	-2.138345	1.281229	0.005642	0.704588
-29.982044	-2.137533	1.286234	0.005641	0.704593
-29.756635	-2.182489	1.291238	0.005599	0.704584
-29.498427	-2.225584	1.296243	0.005551	0.704589
-29.979310	-2.222357	1.301248	0.005640	0.704423
-31.172035	-2.090224	1.306253	0.005862	0.704261
-30.393423	-2.228617	1.311258	0.005718	0.704261
-30.550230	-2.202913	1.316262	0.005747	0.704257
-30.701775	-2.173501	1.321267	0.005775	0.704261
-30.640004	-2.186920	1.326272	0.005764	0.704256
-30.574571	-2.196578	1.331277	0.005752	0.704260
-30.737668	-2.269628	1.336282	0.005782	0.704054
-31.951606	-2.105801	1.341286	0.006008	0.703948
-31.354167	-2.207176	1.346291	0.005897	0.703958
-31.388128	-2.206506	1.351296	0.005903	0.703947
-31.657757	-2.154997	1.356301	0.005954	0.703954
-31.426896	-2.193570	1.361306	0.005911	0.703959
-31.616559	-2.165102	1.366310	0.005946	0.703948
-31.891561	-2.236450	1.371315	0.005998	0.703705
-32.591785	-2.146892	1.376320	0.006128	0.703634
-32.559495	-2.150256	1.381325	0.006122	0.703638
-32.148994	-2.222987	1.386330	0.006046	0.703639
-32.543578	-2.156665	1.391334	0.006119	0.703631
-32.099466	-2.230668	1.396339	0.006037	0.703641
-32.230125	-2.213027	1.401344	0.006061	0.703630
-33.093481	-2.199910	1.406349	0.006222	0.703345
-33.148723	-2.191266	1.411354	0.006232	0.703343
-33.381195	-2.153148	1.416358	0.006275	0.703336
-32.916123	-2.230429	1.421363	0.006189	0.703347
-33.147192	-2.191595	1.426368	0.006232	0.703342
-33.115452	-2.197299	1.431373	0.006226	0.703342
-32.975639	-2.283665	1.436378	0.006200	0.703218
-34.768517	-2.068518	1.441382	0.006534	0.703007
-33.944921	-2.212047	1.446387	0.006381	0.703013
-34.095978	-2.189100	1.451392	0.006409	0.703005
-34.542706	-2.108295	1.456397	0.006492	0.703007
-34.239676	-2.159471	1.461402	0.006436	0.703013
-34.199771	-2.170804	1.466406	0.006429	0.703004
-34.078145	-2.194042	1.471411	0.006406	0.703001
-34.879307	-2.203078	1.476416	0.006555	0.702694
-35.073372	-2.168752	1.481421	0.006592	0.702693
-34.866556	-2.201037	1.486426	0.006553	0.702702
-35.000866	-2.181730	1.491430	0.006578	0.702693
-34.846649	-2.206993	1.496435	0.006550	0.702697
-34.981147	-2.186185	1.501440	0.006575	0.702691
-34.980685	-2.231116	1.506445	0.006575	0.702600
-35.864348	-2.185004	1.511450	0.006739	0.702374
-35.734087	-2.209626	1.516454	0.006715	0.702371
-36.037460	-2.153415	1.521459	0.006772	0.702376
-36.388446	-2.093038	1.526464	0.006837	0.702371
-35.943156	-2.172481	1.531469	0.006754	0.702371
-35.646702	-2.221717	1.536474	0.006699	0.702378
-36.141750	-2.137970	1.541478	0.006791	0.702369
-36.498935	-2.212283	1.546483	0.006858	0.702089
-36.540922	-2.214681	1.551488	0.006866	0.702069
-36.974517	-2.134980	1.556493	0.006947	0.702074
-36.579692	-2.202840	1.561498	0.006873	0.702079
-36.963072	-2.138074	1.566502	0.006945	0.702072
-36.672708	-2.185687	1.571507	0.006891	0.702080
-36.506780	-2.244569	1.576512	0.006860	0.702020
-37.657958	-2.174916	1.581517	0.007074	0.701746
-37.306559	-2.235614	1.586522	0.007009	0.701750
-37.846553	-2.143613	1.591526	0.007110	0.701741
-37.711571	-2.164216	1.596531	0.007085	0.701748
-37.582561	-2.190004	1.601536	0.007061	0.701742
-37.647830	-2.177792	1.606541	0.007073	0.701743
-37.623384	-2.218568	1.611546	0.007068	0.701669
-38.744871	-2.134432	1.616550	0.007277	0.701435
-38.383811	-2.194541	1.621555	0.007210	0.701443
-38.613502	-2.155594	1.626560	0.007253	0.701439
-38.594419	-2.160159	1.631565	0.007249	0.701436
-38.227890	-2.223943	1.636570	0.007181	0.701439
-38.753186	-2.133787	1.641574	0.007279	0.701432
-38.731340	-2.152223	1.646579	0.007275	0.701403
-38.889105	-2.263628	1.651584	0.007305	0.701120
-39.413891	-2.170592	1.656589	0.007402	0.701119
-39.784056	-2.101237	1.661594	0.007471	0.701125
-39.446446	-2.166070	1.666598	0.007409	0.701116
-38.979385	-2.244623	1.671603	0.007322	0.701125
-39.390857	-2.175532	1.676608	0.007398	0.701116
-39.526438	-2.181648	1.681613	0.007424	0.701055
-40.047461	-2.176548	1.686618	0.007521	0.700877
-39.952723	-2.197993	1.691622	0.007503	0.700867
-40.024368	-2.181216	1.696627	0.007517	0.700875
-40.017714	-2.182678	1.701632	0.007515	0.700875
-40.026592	-2.181332	1.706637	0.007517	0.700874
-39.914881	-2.198253	1.711642	0.007496	0.700880
-40.414321	-2.253586	1.716646	0.007590	0.700587
-41.113141	-2.150728	1.721651	0.007720	0.700543
-41.216000	-2.137935	1.726656	0.007739	0.700532
-41.205828	-2.139754	1.731661	0.007737	0.700531
-40.928385	-2.185078	1.736666	0.007686	0.700540
-41.039886	-2.169396	1.741670	0.007706	0.700531
-41.070339	-2.158696	1.746675	0.007712	0.700542
-41.263820	-2.266938	1.751680	0.007748	0.700252
-41.889461	-2.171805	1.756685	0.007865	0.700219
-42.102009	-2.131751	1.761690	0.007904	0.700223
-42.250089	-2.109005	1.766694	0.007932	0.700215
-42.087385	-2.134485	1.771699	0.007902	0.700222
-42.155859	-2.123742	1.776704	0.007915	0.700219
-42.138841	-2.127783	1.781709	0.007912	0.700217
-41.906495	-2.265575	1.786714	0.007868	0.700021
-43.104150	-2.116163	1.791718	0.008091	0.699891
-42.741220	-2.177007	1.796723	0.008024	0.699899
-42.619173	-2.201702	1.801728	0.008001	0.699893
-42.854124	-2.158999	1.806733	0.008045	0.699894
-42.721076	-2.181193	1.811738	0.008020	0.699897
-42.968811	-2.140326	1.816742	0.008067	0.699890
-43.233556	-2.217492	1.821747	0.008116	0.699638
-43.575054	-2.177012	1.826752	0.008180	0.699596
-44.005459	-2.102181	1.831757	0.008260	0.699592
-43.328228	-2.219158	1.836762	0.008134	0.699600
-43.708820	-2.154441	1.841766	0.008205	0.699593
-43.734713	-2.147868	1.846771	0.008210	0.699597
-43.534861	-2.190051	1.851776	0.008173	0.699583
-44.127617	-2.242366	1.856781	0.008283	0.699262
-44.346575	-2.199440	1.861786	0.008324	0.699270
-44.759010	-2.129541	1.866790	0.008401	0.699263
-44.281673	-2.210719	1.871795	0.008312	0.699270
-44.255027	-2.216668	1.876800	0.008307	0.699268
-44.834807	-2.114079	1.881805	0.008415	0.699266
-44.523720	-2.205918	1.886810	0.008357	0.699192
-45.325537	-2.180022	1.891814	0.008507	0.698954
-45.284554	-2.182382	1.896819	0.008499	0.698964
-45.435058	-2.161000	1.901824	0.008527	0.698953
-45.364216	-2.172564	1.906829	0.008514	0.698955
-45.040477	-2.226351	1.911834	0.008454	0.698963
-45.524854	-2.144732	1.916838	0.008544	0.698953
-45.191712	-2.282274	1.921843	0.008482	0.698794
-46.175964	-2.184532	1.926848	0.008666	0.698636
-46.475488	-2.132383	1.931853	0.008721	0.698633
-45.974943	-2.218014	1.936858	0.008628	0.698640
-46.240584	-2.173867	1.941862	0.008678	0.698633
-46.221456	-2.172408	1.946867	0.008674	0.698643
-46.156616	-2.185168	1.951872	0.008662	0.698641
-46.254375	-2.272767	1.956877	0.008681	0.698427
-47.005678	-2.173200	1.961882	0.008821	0.698357
-47.320554	-2.122879	1.966886	0.008879	0.698345
-46.841677	-2.202308	1.971891	0.008790	0.698357
-46.765371	-2.217957	1.976896	0.008776	0.698352
-47.341168	-2.117414	1.981901	0.008883	0.698348
-47.063055	-2.163339	1.986906	0.008832	0.698355
-47.696241	-2.216006	1.991910	0.008950	0.698018
-47.821545	-2.193815	1.996915	0.008973	0.698018
-48.140896	-2.139625	2.001920	0.009032	0.698012

-47.922326	-2.178774	2.011917	0.008992	0.698011
-47.724072	-2.210651	2.021914	0.008955	0.698018
-47.953929	-2.171124	2.031910	0.008998	0.698015
-48.603277	-2.164297	2.041907	0.009119	0.697793
-48.298593	-2.158828	2.051904	0.009063	0.697914
-48.323855	-2.126952	2.061901	0.009067	0.697970
-47.837818	-2.190533	2.071898	0.008977	0.698016
-48.175529	-2.167332	2.081894	0.009040	0.697941
-47.731611	-2.209344	2.091891	0.008958	0.698016
-47.976327	-2.168434	2.101888	0.009003	0.698010
-47.900918	-2.181204	2.111885	0.008989	0.698011
-47.894049	-2.179943	2.121882	0.008988	0.698016
-48.185156	-2.129799	2.131878	0.009043	0.698012
-47.776090	-2.202733	2.141875	0.008967	0.698012
-47.494580	-2.124649	2.151872	0.008914	0.698273
-46.977571	-2.178679	2.161869	0.008818	0.698350
-46.985301	-2.175505	2.171866	0.008820	0.698353
-47.031667	-2.165594	2.181862	0.008829	0.698356
-47.117917	-2.120671	2.191859	0.008845	0.698416
-46.223473	-2.170281	2.201856	0.008678	0.698639
-46.060625	-2.198414	2.211853	0.008648	0.698641
-46.258792	-2.161544	2.221850	0.008685	0.698644
-46.273371	-2.129467	2.231846	0.008688	0.698703
-45.279857	-2.182351	2.241843	0.008503	0.698956
-45.437632	-2.153146	2.251840	0.008533	0.698958
-45.282754	-2.180818	2.261837	0.008504	0.698957
-45.310599	-2.107818	2.271834	0.008509	0.699095
-44.352658	-2.193646	2.281830	0.008331	0.699268
-44.688278	-2.134609	2.291827	0.008394	0.699266
-44.668489	-2.137496	2.301824	0.008390	0.699267
-43.752934	-2.147916	2.311821	0.008220	0.699577
-43.511205	-2.180181	2.321818	0.008175	0.699598
-43.524182	-2.178802	2.331814	0.008178	0.699596
-43.527365	-2.153722	2.341811	0.008179	0.699646
-42.984134	-2.129813	2.351808	0.008077	0.699891
-42.652085	-2.189619	2.361805	0.008016	0.699889
-43.077765	-2.111982	2.371802	0.008095	0.699892
-42.041592	-2.168578	2.381798	0.007902	0.700152
-41.969727	-2.148537	2.391795	0.007889	0.700218
-41.957192	-2.151285	2.401792	0.007887	0.700217
-41.770350	-2.151013	2.411789	0.007852	0.700285
-41.117333	-2.145368	2.421786	0.007731	0.700532
-40.982404	-2.167630	2.431782	0.007706	0.700535
-41.034774	-2.158687	2.441779	0.007716	0.700534
-40.472912	-2.138436	2.451776	0.007611	0.700778
-39.906509	-2.192321	2.461773	0.007506	0.700873
-40.128798	-2.152731	2.471770	0.007548	0.700873
-39.944226	-2.184114	2.481766	0.007513	0.700876
-39.535920	-2.135413	2.491763	0.007438	0.701122
-39.464461	-2.148592	2.501760	0.007424	0.701121
-39.471516	-2.146111	2.511757	0.007426	0.701123
-38.955909	-2.119663	2.521754	0.007330	0.701362
-38.553208	-2.153075	2.531750	0.007255	0.701440
-38.769501	-2.115445	2.541747	0.007296	0.701437
-38.310597	-2.112695	2.551744	0.007210	0.701608
-37.763220	-2.142345	2.561741	0.007108	0.701746
-37.779101	-2.139332	2.571738	0.007112	0.701746
-37.494043	-2.150430	2.581734	0.007059	0.701826
-37.007325	-2.115225	2.591731	0.006968	0.702072
-36.581493	-2.192288	2.601728	0.006889	0.702070
-36.860532	-2.142351	2.611725	0.006941	0.702070
-36.222278	-2.150625	2.621722	0.006822	0.702283
-35.846963	-2.174767	2.631718	0.006753	0.702369
-36.019234	-2.144797	2.641715	0.006785	0.702367
-35.829531	-2.146894	2.651712	0.006750	0.702431
-35.045359	-2.157032	2.661709	0.006604	0.702693
-34.870919	-2.188148	2.671706	0.006572	0.702693
-35.070580	-2.151670	2.681702	0.006609	0.702694
-34.714592	-2.105296	2.691699	0.006543	0.702916
-34.219571	-2.149888	2.701696	0.006451	0.703004
-34.521800	-2.096051	2.711693	0.006507	0.703003
-33.940468	-2.125374	2.721690	0.006399	0.703153
-33.245619	-2.155911	2.731686	0.006270	0.703341
-33.532404	-2.105720	2.741683	0.006323	0.703339
-33.313427	-2.144116	2.751680	0.006283	0.703340
-32.834888	-2.084474	2.761677	0.006194	0.703632
-32.473481	-2.147295	2.771674	0.006127	0.703635
-32.420565	-2.156548	2.781670	0.006117	0.703635
-32.107468	-2.116123	2.791667	0.006059	0.703829
-31.541378	-2.156465	2.801664	0.005954	0.703951
-31.660429	-2.135640	2.811661	0.005976	0.703950
-31.626297	-2.122672	2.821658	0.005970	0.703988
-31.135255	-2.075932	2.831654	0.005878	0.704259
-30.823944	-2.131562	2.841651	0.005821	0.704258
-30.755132	-2.144385	2.851648	0.005808	0.704257
-30.396710	-2.073946	2.861645	0.005741	0.704527
-29.890916	-2.133220	2.871642	0.005647	0.704589
-29.952728	-2.122097	2.881638	0.005659	0.704589
-29.775876	-2.103330	2.891635	0.005626	0.704690
-29.041720	-2.136457	2.901632	0.005490	0.704887
-29.005574	-2.143534	2.911629	0.005483	0.704885
-29.082216	-2.127672	2.921626	0.005497	0.704889
-28.447993	-2.098236	2.931622	0.005379	0.705176
-28.181768	-2.128356	2.941619	0.005330	0.705211
-28.076195	-2.147189	2.951616	0.005311	0.705210
-27.956423	-2.117306	2.961613	0.005288	0.705313
-26.934002	-2.192443	2.971610	0.005098	0.705528
-27.125779	-2.157996	2.981606	0.005134	0.705529
-27.111884	-2.161262	2.991603	0.005132	0.705527
-26.810725	-2.113808	3.001600	0.005076	0.705730
-26.336180	-2.131740	3.011597	0.004987	0.705864
-26.466623	-2.106790	3.021594	0.005012	0.705867
-26.471760	-2.079850	3.031590	0.005013	0.705919
-25.692661	-2.114425	3.041587	0.004868	0.706128
-25.462516	-2.156318	3.051584	0.004825	0.706126
-25.599529	-2.130741	3.061581	0.004851	0.706128
-24.776178	-2.150847	3.071578	0.004698	0.706383
-24.687351	-2.135659	3.081574	0.004682	0.706445
-24.618125	-2.147856	3.091571	0.004669	0.706445
-24.575365	-2.124065	3.101568	0.004661	0.706508
-23.870365	-2.127357	3.111565	0.004530	0.706753
-23.662378	-2.162343	3.121562	0.004491	0.706757
-23.629039	-2.168221	3.131558	0.004485	0.706757
-23.269361	-2.110068	3.141555	0.004418	0.707002
-23.115433	-2.096684	3.151552	0.004390	0.707084
-23.010089	-2.114657	3.161549	0.004370	0.707085
-22.628967	-2.125451	3.171546	0.004300	0.707200
-22.061633	-2.134143	3.181542	0.004194	0.707385
-22.093359	-2.130721	3.191539	0.004200	0.707380
-22.131405	-2.124225	3.201536	0.004207	0.707379
-21.539626	-2.081340	3.211533	0.004097	0.707677
-21.319841	-2.106228	3.221530	0.004057	0.707705
-21.294781	-2.110396	3.231526	0.004052	0.707705
-20.725952	-2.113474	3.241523	0.003946	0.707902
-20.522326	-2.091233	3.251520	0.003908	0.708019
-20.380595	-2.117366	3.261517	0.003882	0.708017
-20.340967	-2.090603	3.271514	0.003875	0.708085
-19.551967	-2.095464	3.281510	0.003728	0.708356
-19.176887	-2.163967	3.291507	0.003659	0.708353
-19.578957	-2.094268	3.301504	0.003734	0.708349
-18.970006	-2.117976	3.311501	0.003620	0.708518
-18.805549	-2.087099	3.321498	0.003590	0.708639
-18.553121	-2.130464	3.331494	0.003543	0.708642
-18.650550	-2.080882	3.341491	0.003561	0.708706
-17.967106	-2.077534	3.351488	0.003434	0.708956
-17.785211	-2.108522	3.361485	0.003400	0.708959
-17.774971	-2.109306	3.371482	0.003399	0.708960
-17.227959	-2.076947	3.381478	0.003297	0.709220
-16.736077	-2.142090	3.391475	0.003206	0.709265
-16.868099	-2.119434	3.401472	0.003230	0.709263
-16.727023	-2.095299	3.411469	0.003204	0.709361
-15.976276	-2.111322	3.421466	0.003065	0.709596
-15.649957	-2.167967	3.431462	0.003004	0.709599
-15.953841	-2.113316	3.441459	0.003061	0.709600
-15.602595	-2.082839	3.451456	0.002995	0.709786
-15.040606	-2.127815	3.461453	0.002891	0.709896
-15.275417	-2.084927	3.471450	0.002935	0.709898
-15.104183	-2.076050	3.481446	0.002903	0.709976
-14.308219	-2.095716	3.491443	0.002755	0.710220
-14.251806	-2.105392	3.501440	0.002745	0.710220
-14.214190	-2.111836	3.511437	0.002738	0.710221
-13.662803	-2.086305	3.521434	0.002635	0.710468
-13.200583	-2.133671	3.531430	0.002549	0.710537
-13.139511	-2.144177	3.541427	0.002538	0.710538
-13.168203	-2.128904	3.551424	0.002544	0.710558
-12.303498	-2.124342	3.561421	0.002383	0.710874
-12.471621	-2.092674	3.571418	0.002414	0.710877
-12.062782	-2.165387	3.581414	0.002338	0.710877
-12.434189	-2.038962	3.591411	0.002408	0.710997
-11.396909	-2.153058	3.601408	0.002215	0.711138
-11.601239	-2.115877	3.611405	0.002253	0.711140
-11.490777	-2.135066	3.621402	0.002232	0.711140
-10.543868	-2.149633	3.631398	0.002056	0.711448
-10.553710	-2.143623	3.641395	0.002058	0.711456
-10.386114	-2.174560	3.651392	0.002027	0.711453
-10.546560	-2.110679	3.661389	0.002057	0.711523
-9.355475	-2.202221	3.671386	0.001836	0.711764
-9.292180	-2.214102	3.681382	0.001824	0.711762
-9.483805	-2.179461	3.691379	0.001860	0.711763
-9.284743	-2.185114	3.701376	0.001823	0.711822
-8.628079	-2.168076	3.711373	0.001701	0.712089
-8.434596	-2.200448	3.721370	0.001665	0.712093
-8.610061	-2.169903	3.731366	0.001698	0.712091
-8.465194	-2.114264	3.741363	0.001671	0.712253
-7.637011	-2.194800	3.751360	0.001517	0.712386
-7.831274	-2.160004	3.761357	0.001553	0.712387
-7.515789	-2.216036	3.771354	0.001494	0.712387
-6.916483	-2.169154	3.781350	0.001383	0.712692
-6.860108	-2.168261	3.791347	0.001373	0.712714
-6.667522	-2.204278	3.801344	0.001337	0.712710
-7.017267	-2.088507	3.811341	0.001402	0.712816
-5.597494	-2.236689	3.821338	0.001138	0.713025
-5.847831	-2.190097	3.831334	0.001185	0.713028
-5.679573	-2.220326	3.841331	0.001154	0.713027
-5.316301	-2.180192	3.851328	0.001086	0.713236
-4.978425	-2.177584	3.861325	0.001023	0.713360
-4.872312	-2.194422	3.871322	0.001004	0.713364
-4.781818	-2.210600	3.881318	0.000987	0.713364
-4.293660	-2.182325	3.891315	0.000896	0.713593
-4.035966	-2.199558	3.901312	0.000848	0.713650
-4.040801	-2.197572	3.911309	0.000850	0.713651
-3.767585	-2.221853	3.921306	0.000799	0.713700
-3.385845	-2.152694	3.931302	0.000728	0.713972
-2.967036	-2.228230	3.941299	0.000650	0.713970
-2.949459	-2.232084	3.951296	0.000647	0.713968
-2.724082	-2.196067	3.961293	0.000605	0.714119
-2.032397	-2.240985	3.971290	0.000476	0.714275
-2.370594	-2.178780	3.981286	0.000540	0.714278
-2.206368	-2.208683	3.991283	0.000509	0.714277
-2.039101	-2.087656	4.001280	0.000478	0.714576
-1.817503	-2.113294	4.011277	0.000437	0.714603
-1.476450	-2.172456	4.021274	0.000374	0.714606
-1.519818	-2.038050	4.031270	0.000382	0.714857
-1.210251	-2.067893	4.041267	0.000324	0.714907
-1.505286	-1.995696	4.051264	0.000379	0.714946
-1.388761	-1.874862	4.061261	0.000358	0.715226
-0.920939	-1.956170	4.071258	0.000271	0.715230
-1.284991	-1.766021	4.081254	0.000339	0.715478
-0.878498	-1.805501	4.091251	0.000263	0.715543
-0.994002	-1.665726	4.101248	0.000285	0.715779
-0.754330	-1.657254	4.111245	0.000240	0.715880
-0.862981	-1.539985	4.121242	0.000261	0.716074
-0.552783	-1.563384	4.131238	0.000203	0.716137
-0.545567	-1.406934	4.141235	0.000202	0.716449
-0.645677	-1.336820	4.151232	0.000220	0.716552
-0.703747	-1.224245	4.161229	0.000231	0.716755
-0.867889	-1.051474	4.171226	0.000262	0.717038
-0.482276	-1.025999	4.181222	0.000190	0.717224
-0.392007	-0.948959	4.191219	0.000173	0.717408
-0.302912	-0.818238	4.201216	0.000157	0.717698
-0.398438	-0.678303	4.211213	0.000175	0.717940
-0.426920	-0.548331	4.221210	0.000180	0.718187
-0.207143	-0.455408	4.231206	0.000139	0.718447
-0.368442	-0.296743	4.241203	0.000169	0.718704
-0.398560	-0.144959	4.251200	0.000175	0.718992
-0.269650	-0.022113	4.261197	0.000151	0.719280
0.000000	0.139108	4.271194	0.000101	0.719692

-0.178664	0.777892	4.276198	0.000134	0.720887
0.020638	1.999597	4.281203	0.000096	0.723357
0.226297	3.813633	4.286208	0.000057	0.726977
0.356681	6.194675	4.291213	0.000031	0.731654
0.537485	9.077054	4.296218	-0.000005	0.737283
0.980250	12.381076	4.301222	-0.000089	0.743764
1.587958	16.125597	4.306227	-0.000205	0.751076
1.824592	20.337923	4.311232	-0.000251	0.759069
2.163386	24.923580	4.316237	-0.000317	0.767702
2.857364	29.826642	4.321242	-0.000450	0.776934
3.232660	35.121374	4.326246	-0.000523	0.786662
3.886464	40.704342	4.331251	-0.000648	0.796872
4.191211	46.633468	4.336256	-0.000709	0.807452
4.431797	52.867784	4.341261	-0.000758	0.818405
4.888245	59.333377	4.346266	-0.000847	0.829673
5.164861	66.045698	4.351270	-0.000902	0.841153
5.962231	72.897534	4.356275	-0.001055	0.852863
7.319974	79.856905	4.361280	-0.001313	0.864753
8.296893	87.091690	4.366285	-0.001499	0.876817
9.485832	94.476276	4.371290	-0.001725	0.889016
11.669854	101.846451	4.376294	-0.002137	0.901301
12.201786	109.688274	4.381299	-0.002241	0.913702
12.760208	117.620598	4.386304	-0.002350	0.926082
13.633058	125.628146	4.391309	-0.002517	0.938496
14.376476	133.765450	4.396314	-0.002661	0.950907
15.423200	141.923985	4.401318	-0.002861	0.963266
16.343751	150.210370	4.406323	-0.003038	0.975622
17.084395	158.592049	4.411328	-0.003181	0.987915
17.878291	167.029780	4.416333	-0.003335	1.000149
18.681541	175.502515	4.421338	-0.003490	1.012286
19.294971	184.035238	4.426342	-0.003609	1.024316
20.307376	192.562161	4.431347	-0.003803	1.036293
21.114849	201.135643	4.436352	-0.003959	1.048147
22.218559	209.704604	4.441357	-0.004170	1.059931
22.985781	218.356835	4.446362	-0.004319	1.071618
23.735783	226.999938	4.451366	-0.004464	1.083162
24.586728	235.638144	4.456371	-0.004628	1.094601
25.126539	244.317102	4.461376	-0.004734	1.105904
25.698869	253.006719	4.466381	-0.004846	1.117113
26.493614	261.635786	4.471386	-0.005000	1.128183
27.609619	270.222100	4.476390	-0.005213	1.139160
28.426013	278.885048	4.481395	-0.005370	1.150062
29.193185	287.539383	4.486400	-0.005519	1.160841
29.567709	296.217184	4.491405	-0.005594	1.171468
30.516600	304.792794	4.496410	-0.005776	1.181994
31.303376	313.389511	4.501414	-0.005928	1.192419
31.678331	322.036905	4.506419	-0.006004	1.202730
32.160019	330.653836	4.511424	-0.006099	1.212939
32.526560	339.271657	4.516429	-0.006173	1.223040
33.394579	347.820988	4.521434	-0.006340	1.233078
33.916575	356.369377	4.526438	-0.006443	1.242967
34.484162	364.923390	4.531443	-0.006554	1.252792
34.892028	373.468738	4.536448	-0.006635	1.262500
35.183732	382.032626	4.541453	-0.006695	1.272133
35.651404	390.538235	4.546458	-0.006788	1.281662
36.186010	399.015649	4.551462	-0.006893	1.291102
37.177823	407.416274	4.556467	-0.007083	1.300473
37.737050	415.933671	4.561472	-0.007192	1.309824
38.274199	424.448065	4.566477	-0.007298	1.319102
39.283906	432.789701	4.571482	-0.007491	1.328214
39.620060	441.245670	4.576486	-0.007559	1.337266
40.066940	449.657837	4.581491	-0.007648	1.346230
40.511702	458.084787	4.586496	-0.007736	1.355150
41.291510	466.414864	4.591501	-0.007887	1.363968
41.764781	474.827138	4.596506	-0.007980	1.372762
41.940217	483.240076	4.601510	-0.008018	1.381450
42.650215	491.587412	4.606515	-0.008156	1.390106
43.241230	499.941105	4.611520	-0.008271	1.398696
43.828148	508.253851	4.616525	-0.008386	1.407190
44.283780	516.614073	4.621530	-0.008476	1.415659
44.648635	524.957280	4.626534	-0.008549	1.424046
45.284327	533.281596	4.631539	-0.008673	1.432409
45.710889	541.598755	4.636544	-0.008758	1.440683
46.343570	549.892156	4.641549	-0.008881	1.448919
46.893784	558.216275	4.646554	-0.008989	1.457124
47.239818	566.527897	4.651558	-0.009059	1.465239
47.730632	574.883336	4.656563	-0.009155	1.473374
48.341072	583.145479	4.661568	-0.009274	1.481394
48.840505	591.421556	4.666573	-0.009373	1.489367
49.127647	599.741935	4.671578	-0.009431	1.497305
49.736078	607.964593	4.676582	-0.009550	1.505160
50.304169	616.238123	4.681587	-0.009661	1.513014
50.843763	624.472110	4.686592	-0.009767	1.520787
51.342026	632.720996	4.691597	-0.009865	1.528527
51.873944	640.989822	4.696602	-0.009969	1.536252
52.199347	649.241615	4.701606	-0.010035	1.543892
52.705142	657.508420	4.706611	-0.010135	1.551534
53.090192	665.756494	4.711616	-0.010212	1.559104
53.396905	673.998114	4.716621	-0.010274	1.566619
53.786951	682.257789	4.721626	-0.010352	1.574128
54.214873	690.465226	4.726630	-0.010437	1.581559
54.829270	698.671990	4.731635	-0.010557	1.588981
55.315356	706.896143	4.736640	-0.010652	1.596365
55.806284	715.090712	4.741645	-0.010749	1.603690
56.412648	723.299519	4.746650	-0.010867	1.611011
56.683807	731.537349	4.751654	-0.010923	1.618276
57.608040	739.672579	4.756659	-0.011100	1.625511
57.977691	747.959510	4.761664	-0.011175	1.632767
58.173943	756.192358	4.766669	-0.011216	1.639921
58.788448	764.348821	4.771674	-0.011336	1.647036
59.358252	772.530344	4.776678	-0.011447	1.654135
59.580658	780.764121	4.781683	-0.011494	1.661200
60.150708	788.925998	4.786688	-0.011605	1.668222
60.565056	797.134145	4.791693	-0.011688	1.675232
61.194133	805.286227	4.796698	-0.011810	1.682195
61.433443	813.491840	4.801702	-0.011860	1.689122
61.949837	821.683158	4.806707	-0.011962	1.696044
62.622349	829.814069	4.811712	-0.012092	1.702909
62.760632	838.051254	4.816717	-0.012123	1.709765
63.291276	846.234938	4.821722	-0.012227	1.716599
63.614055	854.391629	4.826726	-0.012292	1.723358
64.191255	862.535414	4.831731	-0.012405	1.730112
64.427290	870.742760	4.836736	-0.012454	1.736847
64.612764	878.926557	4.841741	-0.012494	1.743531
65.197439	887.073356	4.846746	-0.012608	1.750210
65.648347	895.224581	4.851750	-0.012697	1.756851
66.229373	903.349504	4.856755	-0.012811	1.763461
66.573199	911.522005	4.861760	-0.012880	1.770055
67.064953	919.677067	4.866765	-0.012977	1.776628
67.550894	927.831124	4.871770	-0.013073	1.783176
68.087713	935.980537	4.876774	-0.013178	1.789702
68.465654	944.194787	4.881779	-0.013253	1.796236
68.632177	952.344511	4.886784	-0.013290	1.802670
69.314203	960.440621	4.891789	-0.013422	1.809101
69.644052	968.613417	4.896794	-0.013489	1.815527
70.054750	976.731340	4.901798	-0.013570	1.821897
70.499302	984.862999	4.906803	-0.013658	1.828259
71.047033	993.008365	4.911808	-0.013765	1.834622
71.318288	1001.155225	4.916813	-0.013821	1.840932
71.915285	1009.278082	4.921818	-0.013938	1.847239
72.475782	1017.408315	4.926822	-0.014047	1.853526
73.104271	1025.530661	4.931827	-0.014169	1.859794
73.487509	1033.680036	4.936832	-0.014246	1.866033
73.851791	1041.853969	4.941837	-0.014319	1.872267
74.409090	1049.990246	4.946842	-0.014428	1.878474
74.665171	1058.110490	4.951846	-0.014481	1.884614
74.987448	1066.247612	4.956851	-0.014546	1.890754
75.768684	1074.329658	4.961856	-0.014697	1.896885
76.214965	1082.438609	4.966861	-0.014785	1.902978
76.713401	1090.573647	4.971866	-0.014883	1.909077
77.093662	1098.708913	4.976870	-0.014959	1.915143
77.770266	1106.797170	4.981875	-0.015090	1.921188
77.700710	1114.995642	4.986880	-0.015083	1.927213
77.898175	1123.139418	4.991885	-0.015125	1.933208
78.481942	1131.235988	4.996890	-0.015239	1.939192
78.818046	1139.339559	5.001894	-0.015306	1.945136
79.033089	1147.524694	5.006899	-0.015352	1.951108
79.571360	1155.637027	5.011904	-0.015457	1.957043
79.816015	1163.734016	5.016909	-0.015508	1.962918
79.889604	1171.884543	5.021914	-0.015527	1.968795
80.194708	1179.984223	5.026918	-0.015589	1.974643
80.869690	1188.036436	5.031923	-0.015720	1.980480
81.274462	1196.131546	5.036928	-0.015800	1.986301
81.616934	1204.249483	5.041933	-0.015869	1.992114
82.183323	1212.337470	5.046938	-0.015980	1.997913
82.480607	1220.431473	5.051942	-0.016041	2.003670
82.863151	1228.550575	5.056947	-0.016117	2.009438
83.414568	1236.647910	5.061952	-0.016225	2.015191
83.842130	1244.734563	5.066957	-0.016310	2.020908
84.250090	1252.861901	5.071962	-0.016391	2.026635
84.455514	1261.007236	5.076966	-0.016434	2.032337
84.877802	1269.107535	5.081971	-0.016518	2.038014
85.123972	1277.209333	5.086976	-0.016569	2.043658
85.277981	1285.328740	5.091981	-0.016603	2.049290
85.519700	1293.463660	5.096986	-0.016653	2.054925
86.044586	1301.508095	5.101990	-0.016756	2.060512
86.401850	1309.598613	5.106995	-0.016828	2.066097
86.995265	1317.683938	5.112000	-0.016944	2.071688
87.413301	1325.780731	5.117005	-0.017027	2.077254
87.763304	1333.880088	5.122010	-0.017097	2.082800
88.036392	1341.967365	5.127014	-0.017153	2.088315
88.500496	1350.074152	5.132019	-0.017245	2.093848
88.826704	1358.171814	5.137024	-0.017311	2.099346
88.924312	1366.282522	5.142029	-0.017334	2.104817
89.276877	1374.413167	5.147034	-0.017405	2.110311
89.532450	1382.555027	5.152038	-0.017458	2.115789
89.787738	1390.613897	5.157043	-0.017510	2.121197
90.285361	1398.670374	5.162048	-0.017608	2.126614
90.673349	1406.734862	5.167053	-0.017686	2.132011
91.197524	1414.810204	5.172058	-0.017789	2.137414
91.260152	1422.914920	5.177062	-0.017805	2.142780
91.615614	1430.994754	5.182067	-0.017877	2.148143
91.989908	1439.107574	5.187072	-0.017952	2.153516
92.013124	1447.207754	5.192077	-0.017961	2.158835
92.445426	1455.266727	5.197082	-0.018047	2.164152
92.617616	1463.356343	5.202086	-0.018084	2.169451
93.159359	1471.431068	5.207091	-0.018190	2.174762
93.516274	1479.503627	5.212096	-0.018262	2.180042
93.714896	1487.580641	5.217101	-0.018304	2.185297
93.871039	1495.743444	5.222106	-0.018338	2.190590
94.095989	1503.837667	5.227110	-0.018385	2.195834
94.857406	1511.822216	5.232115	-0.018532	2.201042
95.259383	1519.898370	5.237120	-0.018612	2.206265
95.466179	1527.999749	5.242125	-0.018656	2.211473
95.953322	1536.071663	5.247130	-0.018752	2.216676
96.369462	1544.126067	5.252134	-0.018835	2.221849
96.733608	1552.211763	5.257139	-0.018908	2.227025
96.822026	1560.354432	5.262144	-0.018929	2.232200
97.144319	1568.416225	5.267149	-0.018995	2.237333
97.316568	1576.503882	5.272154	-0.019032	2.242458
97.484387	1584.575336	5.277158	-0.019068	2.247560
97.812175	1592.666836	5.282163	-0.019134	2.252677
98.108532	1600.758438	5.287168	-0.019195	2.257779
98.336395	1608.819415	5.292173	-0.019242	2.262845
98.786671	1616.889046	5.297178	-0.019331	2.267924
99.149761	1625.014503	5.302182	-0.019404	2.273019
99.332812	1633.108968	5.307187	-0.019444	2.278068
99.608224	1641.148069	5.312192	-0.019500	2.283079
100.017283	1649.167417	5.317197	-0.019581	2.288078
100.665143	1657.219527	5.322202	-0.019707	2.293107
100.669214	1665.321523	5.327206	-0.019713	2.298101
100.869828	1673.383418	5.332211	-0.019756	2.303076
101.177294	1681.465048	5.337216	-0.019818	2.308061
101.361972	1689.551587	5.342221	-0.019858	2.313028
101.467787	1697.647252	5.347226	-0.019883	2.317984
101.812186	1705.667259	5.352230	-0.019952	2.322902
102.149223	1713.726575	5.357235	-0.020020	2.327833
102.352032	1721.827420	5.362240	-0.020063	2.332768
102.479118	1729.903248	5.367245	-0.020092	2.337672
103.076212	1737.932830	5.372250	-0.020208	2.342575
103.200936	1746.017017	5.377254	-0.020236	2.347462
103.622682	1754.098181	5.382259	-0.020320	2.352362
104.069156	1762.150231	5.387264	-0.020408	2.357236
104.301967	1770.197274	5.392269	-0.020457	2.362079
104.641164	1778.268339	5.397274	-0.020525	2.366935
104.738904	1786.356265	5.402278	-0.020549	2.371772
105.093164	1794.421843	5.407283	-0.020620	2.376606
105.123224	1802.508972	5.412288	-0.020631	2.381418
105.593527	1810.528738	5.417293	-0.020723	2.386214
105.935639	1818.612723	5.422298	-0.020792	2.391029
105.860723	1826.725606	5.427302	-0.020783	2.395818
106.209323	1834.748640	5.432307	-0.020854	2.400578
106.631455	1842.773795	5.437312	-0.020937	2.405336
106.772097	1850.868529	5.442317	-0.020969	2.410102
107.118273	1858.960885	5.447322	-0.021038	2.414874
107.337897	1867.008838	5.452326	-0.021084	2.419601
107.467318	1875.094795	5.457331	-0.021114	2.424334
107.929402	1883.125311	5.462336	-0.021205	2.429051
108.315552	1891.237907	5.467341	-0.021282	2.433800
108.600233	1899.298723	5.472346	-0.021340	2.438502
108.598913	1907.346890	5.477350	-0.021345	2.443166
108.831557	1915.391032	5.482355	-0.021394	2.447837
109.209290	1923.451409	5.487360	-0.021469	2.452518
109.476187	1931.482854	5.492365	-0.021524	2.457166
109.737622	1939.555669	5.497370	-0.021578	2.461829
109.837765	1947.617408	5.502374	-0.021602	2.466464
110.045334	1955.683368	5.507379	-0.021645	2.471101
110.448275	1963.756923	5.512384	-0.021726	2.475748
110.295769	1971.826202	5.517389	-0.021702	2.480342
110.818860	1979.836853	5.522394	-0.021805	2.484945
110.859617	1987.903005	5.527398	-0.021818	2.489535
110.866899	1996.019519	5.532403	-0.021824	2.494142
111.290582	2004.052256	5.537408	-0.021908	2.498724
111.478171	2012.087125	5.542413	-0.021949	2.503282
111.807783	2020.144193	5.547418	-0.022015	2.507854
111.825726	2028.255472	5.552422	-0.022024	2.512426
112.280028	2036.294067	5.557427	-0.022113	2.516980
112.543381	2044.316362	5.562432	-0.022168	2.521503
112.813224	2052.350170	5.567437	-0.022223	2.526024
113.296096	2060.373527	5.572442	-0.022318	2.530547
113.682919	2068.447322	5.577446	-0.022395	2.535083
113.713462	2076.515964	5.582451	-0.022406	2.539583
114.124075	2084.544358	5.587456	-0.022488	2.544079
114.435236	2092.597614	5.592461	-0.022551	2.548574
114.730382	2100.687048	5.597466	-0.022611	2.553080
114.826624	2108.748148	5.602470	-0.022634	2.557548
115.177960	2116.779245	5.607475	-0.022705	2.562010
115.426001	2124.851785	5.612480	-0.022756	2.566479
115.611168	2132.903359	5.617485	-0.022796	2.570925
115.946463	2140.987031	5.622490	-0.022863	2.575391
116.154822	2149.014349	5.627494	-0.022907	2.579809
116.279474	2157.066649	5.632499	-0.022936	2.584228
116.618028	2165.128850	5.637504	-0.023004	2.588660
116.782398	2173.323065	5.642509	-0.023040	2.593143
117.030195	2181.394409	5.647514	-0.023091	2.597558
117.130337	2189.387209	5.652518	-0.023115	2.601913
117.637059	2197.364948	5.657523	-0.023214	2.606279
117.711741	2205.416479	5.662528	-0.023233	2.610649
117.929092	2213.456901	5.667533	-0.023279	2.615016
118.380723	2221.483863	5.672538	-0.023368	2.619383
118.598929	2229.506490	5.677542	-0.023414	2.623725
118.740830	2237.574609	5.682547	-0.023446	2.628079
119.045758	2245.636656	5.687552	-0.023508	2.632434
119.242362	2253.667089	5.692557	-0.023549	2.636757
119.477619	2261.743389	5.697562	-0.023598	2.641100
119.520003	2269.778565	5.702566	-0.023611	2.645402
119.939569	2277.793743	5.707571	-0.023695	2.649710
120.167286	2285.887325	5.712576	-0.023742	2.654041
120.187143	2293.914041	5.717581	-0.023751	2.658315
120.402322	2302.000393	5.722586	-0.023796	2.662627
120.703673	2310.021768	5.727590	-0.023858	2.666903
120.993942	2318.091758	5.732595	-0.023917	2.671197
121.158762	2326.183657	5.737600	-0.023953	2.675487
121.538593	2334.159023	5.742605	-0.024029	2.679723
121.971778	2342.190556	5.747610	-0.024114	2.683985
122.220131	2350.241440	5.752614	-0.024166	2.688239
122.582364	2358.289697	5.757619	-0.024239	2.692492
122.856673	2366.372214	5.762624	-0.024295	2.696750
122.961497	2374.397418	5.767629	-0.024319	2.700961
123.373428	2382.441923	5.772634	-0.024401	2.705195
123.422868	2390.497288	5.777638	-0.024416	2.709405
123.584330	2398.579367	5.782643	-0.024451	2.713629
123.827043	2406.609817	5.787648	-0.024501	2.717825
124.029603	2414.637781	5.792653	-0.024544	2.722011
124.517611	2422.653242	5.797658	-0.024640	2.726201
124.734010	2430.694342	5.802662	-0.024686	2.730382
124.807894	2438.786564	5.807667	-0.024705	2.734573
124.971290	2446.840118	5.812672	-0.024740	2.738744
125.234839	2454.845739	5.817677	-0.024794	2.742890
125.331512	2462.920355	5.822682	-0.024818	2.747054
125.506094	2470.985338	5.827686	-0.024855	2.751213
125.783407	2479.100420	5.832691	-0.024912	2.755396
126.075345	2487.094049	5.837696	-0.024972	2.759513
126.197953	2495.090373	5.842701	-0.025000	2.763614
126.505317	2503.130168	5.847706	-0.025062	2.767742
126.754398	2511.152854	5.852710	-0.025114	2.771852
127.081597	2519.202991	5.857715	-0.025180	2.775974
127.407363	2527.232300	5.862720	-0.025245	2.780079
127.457074	2535.273840	5.867725	-0.025260	2.784169
127.785764	2543.350843	5.872730	-0.025326	2.788286
128.250933	2551.379741	5.877734	-0.025418	2.792381
128.377321	2559.441414	5.882739	-0.025447	2.796467
128.515757	2567.485112	5.887744	-0.025478	2.800538
128.683580	2575.482703	5.892749	-0.025514	2.804582
129.193940	2583.530610	5.897754	-0.025614	2.808666
129.252383	2591.595934	5.902758	-0.025630	2.812726
129.511422	2599.639955	5.907763	-0.025684	2.816780
129.562152	2607.704655	5.912768	-0.025698	2.820828
129.728994	2615.720267	5.917773	-0.025735	2.824851
129.997268	2623.787045	5.922778	-0.025790	2.828901
130.351865	2631.827534	5.927782	-0.025861	2.832936
130.428952	2639.891876	5.932787	-0.025880	2.836961
130.819620	2647.885008	5.937792	-0.025958	2.840963
130.879005	2655.898333	5.942797	-0.025975	2.844951
131.317763	2663.946651	5.947802	-0.026061	2.848972
131.522744	2672.005307	5.952806	-0.026105	2.852979
131.840782	2680.038038	5.957811	-0.026169	2.856974
132.301440	2688.079387	5.962816	-0.026260	2.860975
132.352133	2696.098658	5.967821	-0.026275	2.864938
132.727466	2704.150259	5.972826	-0.026350	2.868928
133.019765	2712.209270	5.977830	-0.026409	2.872912
133.421280	2720.247075	5.982835	-0.026489	2.876886
133.438757	2728.313684	5.987840	-0.026498	2.880848
133.687947	2736.301210	5.992845	-0.026549	2.884778
134.071098	2744.357590	5.997850	-0.026626	2.888743
134.035617	2752.442403	6.002854	-0.026624	2.892694
134.141484	2760.517454	6.007859	-0.026649	2.896643
134.466021	2768.523627	6.012864	-0.026715	2.900565
134.770422	2776.496852	6.017869	-0.026777	2.904464
135.065020	2784.591255	6.022874	-0.026837	2.908416
135.341125	2792.669924	6.027878	-0.026893	2.912354
135.509705	2800.735439	6.032883	-0.026930	2.916275
135.739436	2808.751008	6.037888	-0.026978	2.920169
135.914277	2816.715606	6.042893	-0.027015	2.924031
136.166191	2824.771004	6.047898	-0.027068	2.927935
136.286333	2832.809594	6.052902	-0.027095	2.931819
136.167079	2840.884365	6.057907	-0.027078	2.935703
136.731351	2848.877207	6.062912	-0.027188	2.939578
136.836794	2856.893685	6.067917	-0.027213	2.943435
136.999375	2864.951656	6.072922	-0.027248	2.947310
137.041771	2873.005955	6.077926	-0.027262	2.951172
137.284045	2881.057070	6.082931	-0.027312	2.955038
137.552898	2889.078088	6.087936	-0.027367	2.958885
137.728431	2897.062148	6.092941	-0.027405	2.962705
138.161188	2905.114818	6.097946	-0.027491	2.966566
138.114254	2913.189644	6.102950	-0.027487	2.970408
138.166505	2921.253774	6.107955	-0.027502	2.974245
138.702982	2929.235153	6.112960	-0.027607	2.978062
138.985956	2937.267281	6.117965	-0.027665	2.981886
139.071317	2945.332897	6.122970	-0.027686	2.985710
139.317452	2953.347569	6.127974	-0.027737	2.989514
139.515512	2961.425957	6.132979	-0.027779	2.993340
139.691339	2969.472125	6.137984	-0.027817	2.997145
139.727365	2977.504943	6.142989	-0.027829	3.000932
140.072353	2985.510024	6.147994	-0.027898	3.004717
140.237019	2993.545041	6.152998	-0.027934	3.008502
140.180811	3001.604837	6.158003	-0.027929	3.012282
140.675125	3009.630297	6.163008	-0.028026	3.016069
140.838550	3017.634049	6.168013	-0.028061	3.019825
140.913575	3025.699850	6.173018	-0.028081	3.023601
141.121301	3033.733841	6.178022	-0.028124	3.027364
141.304929	3041.789159	6.183027	-0.028164	3.031130
141.709517	3049.820901	6.188032	-0.028244	3.034892
141.865566	3057.821480	6.193037	-0.028278	3.038622
142.075377	3065.854641	6.198042	-0.028323	3.042366
142.282387	3073.879932	6.203046	-0.028366	3.046101
142.313039	3081.932709	6.208051	-0.028377	3.049836
142.787434	3089.982740	6.213056	-0.028471	3.053586
142.962162	3098.002121	6.218061	-0.028508	3.057303
143.193338	3106.039093	6.223066	-0.028557	3.061027
143.313810	3114.035694	6.228070	-0.028584	3.064721
143.611598	3122.101855	6.233075	-0.028645	3.068452
143.662606	3130.218101	6.238080	-0.028660	3.072190
143.833159	3138.285200	6.243085	-0.028697	3.075906
144.162529	3146.239185	6.248090	-0.028763	3.079573
144.600505	3154.219059	6.253094	-0.028850	3.083253
144.719516	3162.266221	6.258099	-0.028877	3.086944
144.938787	3170.332756	6.263104	-0.028923	3.090644
145.400040	3178.308785	6.268109	-0.029014	3.094310
145.611782	3186.359328	6.273114	-0.029059	3.097993
145.625057	3194.414145	6.278118	-0.029066	3.101665
145.992062	3202.416299	6.283123	-0.029140	3.105325
146.218771	3210.483343	6.288128	-0.029187	3.109004
146.189682	3218.534713	6.293133	-0.029187	3.112659
146.518397	3226.604637	6.298138	-0.029253	3.116335
146.749971	3234.569144	6.303142	-0.029301	3.119955
146.883159	3242.589371	6.308147	-0.029331	3.123591
147.112291	3250.637843	6.313152	-0.029379	3.127239
147.275962	3258.664951	6.318157	-0.029415	3.130871
147.600580	3266.726451	6.323162	-0.029481	3.134521
147.738316	3274.764612	6.328166	-0.029511	3.138148
147.903886	3282.765675	6.333171	-0.029547	3.141756
148.209985	3290.803940	6.338176	-0.029609	3.145382
148.162237	3298.845930	6.343181	-0.029606	3.148990
148.531751	3306.902330	6.348186	-0.029680	3.152619
148.717740	3314.952626	6.353190	-0.029720	3.156233
148.780208	3322.949557	6.358195	-0.029736	3.159813
149.017145	3330.968708	6.363200	-0.029786	3.163407
149.322959	3338.979928	6.368205	-0.029848	3.166996
149.413877	3347.040804	6.373210	-0.029870	3.170594
149.637505	3355.074928	6.378214	-0.029917	3.174181
149.617066	3363.110176	6.383219	-0.029918	3.177754
150.067216	3371.137334	6.388224	-0.030007	3.181340
150.191099	3379.124855	6.393229	-0.030035	3.184891
150.337255	3387.197436	6.398234	-0.030067	3.188476
150.777037	3395.222902	6.403238	-0.030155	3.192048
150.814556	3403.281828	6.408243	-0.030167	3.195614
151.107762	3411.295045	6.413248	-0.030226	3.199167
151.216621	3419.282456	6.418253	-0.030252	3.202697
151.310980	3427.359473	6.423258	-0.030275	3.206262
151.353123	3435.385212	6.428262	-0.030288	3.209798
151.882219	3443.398001	6.433267	-0.030391	3.213344
152.063522	3451.462631	6.438272	-0.030430	3.216895
152.073632	3459.463398	6.443277	-0.030437	3.220407
152.349361	3467.492165	6.448282	-0.030494	3.223939
152.631921	3475.534230	6.453286	-0.030551	3.227472
152.796467	3483.588426	6.458291	-0.030587	3.231002
153.111590	3491.686804	6.463296	-0.030651	3.234554
153.413603	3499.638740	6.468301	-0.030713	3.238037
153.602998	3507.662864	6.473306	-0.030753	3.241543
153.483193	3515.670635	6.478310	-0.030736	3.245026
153.914896	3523.672580	6.483315	-0.030821	3.248525
154.402413	3531.738596	6.488320	-0.030917	3.252050
154.491911	3539.771107	6.493325	-0.030939	3.255541
154.480851	3547.794877	6.498330	-0.030942	3.259020
154.761809	3555.800450	6.503334	-0.031000	3.262499
154.951139	3563.839698	6.508339	-0.031040	3.265985
155.159361	3571.877961	6.513344	-0.031084	3.269468
155.316363	3579.931740	6.518349	-0.031118	3.272952
155.678508	3587.982778	6.523354	-0.031191	3.276439
155.899232	3595.959712	6.528358	-0.031237	3.279885
156.109604	3603.985998	6.533363	-0.031282	3.283348
156.346519	3612.030093	6.538368	-0.031331	3.286816
156.557870	3620.020384	6.543373	-0.031375	3.290256
156.785808	3628.102833	6.548378	-0.031423	3.293732
156.838604	3636.123658	6.553382	-0.031438	3.297172
157.091330	3644.141556	6.558387	-0.031490	3.300615
156.994984	3652.202062	6.563392	-0.031477	3.304059
157.194228	3660.211689	6.568397	-0.031520	3.307489
157.617701	3668.252233	6.573402	-0.031604	3.310937
157.639777	3676.329672	6.578406	-0.031613	3.314381
157.906685	3684.330045	6.583411	-0.031668	3.317799
158.263936	3692.316137	6.588416	-0.031739	3.321210
158.447831	3700.302387	6.593421	-0.031779	3.324612
158.717213	3708.351919	6.598426	-0.031834	3.328040
158.971816	3716.406029	6.603430	-0.031887	3.331466
159.269086	3724.436810	6.608435	-0.031947	3.334880
159.317646	3732.474091	6.613440	-0.031961	3.338283
159.452164	3740.506939	6.618445	-0.031992	3.341685
160.138789	3748.479304	6.623450	-0.032125	3.345078
160.293920	3756.509937	6.628454	-0.032159	3.348473
160.436387	3764.573608	6.633459	-0.032190	3.351877
160.715683	3772.650046	6.638464	-0.032248	3.355289
160.724667	3780.624508	6.643469	-0.032254	3.358644
160.996018	3788.661676	6.648474	-0.032310	3.362032
161.186422	3796.689485	6.653478	-0.032351	3.365409
161.595042	3804.665808	6.658483	-0.032432	3.368769
161.511132	3812.766180	6.663488	-0.032421	3.372160
161.719960	3820.799722	6.668493	-0.032465	3.375531
161.912954	3828.821082	6.673498	-0.032507	3.378892
162.161739	3836.857010	6.678502	-0.032558	3.382258
162.252539	3844.854566	6.683507	-0.032580	3.385598
162.804741	3852.893769	6.688512	-0.032688	3.388969
162.909449	3860.966959	6.693517	-0.032713	3.392336
163.045037	3869.038872	6.698522	-0.032743	3.395699
163.146765	3876.997711	6.703526	-0.032767	3.399011
163.520961	3884.981429	6.708531	-0.032842	3.402339
163.631598	3893.022258	6.713536	-0.032868	3.405679
163.833924	3901.034763	6.718541	-0.032911	3.409007
164.197938	3909.071937	6.723546	-0.032984	3.412347
164.422795	3917.114355	6.728550	-0.033031	3.415681
164.522244	3925.095749	6.733555	-0.033054	3.418983
164.765564	3933.158536	6.738560	-0.033105	3.422319
164.955932	3941.163239	6.743565	-0.033145	3.425627
165.314067	3949.184738	6.748570	-0.033217	3.428944
165.263116	3957.265912	6.753574	-0.033213	3.432269
165.426036	3965.301721	6.758579	-0.033248	3.435579
165.844336	3973.274357	6.763584	-0.033331	3.438868
165.774096	3981.312838	6.768589	-0.033323	3.442165
166.250602	3989.302437	6.773594	-0.033417	3.445457
166.435565	3997.357825	6.778598	-0.033457	3.448763
166.500394	4005.406314	6.783603	-0.033474	3.452059
166.782216	4013.445812	6.788608	-0.033532	3.455355
166.931321	4021.457911	6.793613	-0.033565	3.458632
166.977069	4029.501282	6.798618	-0.033578	3.461916
167.186127	4037.513972	6.803622	-0.033623	3.465189
167.595145	4045.537558	6.808627	-0.033704	3.468471
167.828136	4053.587557	6.813632	-0.033752	3.471754
167.860013	4061.638211	6.818637	-0.033763	3.475028
168.311716	4069.610926	6.823642	-0.033853	3.478280
168.559917	4077.645119	6.828646	-0.033904	3.481548
168.602140	4085.629248	6.833651	-0.033917	3.484786
168.744126	4093.695508	6.838656	-0.033949	3.488057
168.971551	4101.700181	6.843661	-0.033996	3.491303
168.960436	4109.765850	6.848666	-0.033999	3.494563
169.268377	4117.779348	6.853670	-0.034062	3.497809
169.537936	4125.770913	6.858675	-0.034117	3.501042
169.694459	4133.785747	6.863680	-0.034151	3.504277
169.793189	4141.826505	6.868685	-0.034175	3.507519
169.928773	4149.847063	6.873690	-0.034205	3.510750
170.006968	4157.927678	6.878694	-0.034225	3.514000
170.220996	4165.931491	6.883699	-0.034270	3.517221
170.575812	4173.946741	6.888704	-0.034341	3.520448
170.850024	4181.937500	6.893709	-0.034397	3.523660
171.053517	4189.987092	6.898714	-0.034441	3.526890
171.135143	4198.008160	6.903718	-0.034461	3.530102
171.430318	4206.060999	6.908723	-0.034521	3.533330
171.832482	4214.096823	6.913728	-0.034601	3.536552
171.658573	4222.117130	6.918733	-0.034574	3.539747
171.805302	4230.126729	6.923738	-0.034606	3.542944
171.843895	4238.152546	6.928742	-0.034619	3.546142
172.054647	4246.175086	6.933747	-0.034663	3.549341
172.338577	4254.304770	6.938752	-0.034721	3.552581
172.519305	4262.338835	6.943757	-0.034760	3.555778
172.791694	4270.266368	6.948762	-0.034816	3.558932
172.888544	4278.305457	6.953766	-0.034839	3.562123
173.311824	4286.270107	6.958771	-0.034923	3.565290
173.656437	4294.307817	6.963776	-0.034992	3.568482
173.528532	4302.361582	6.968781	-0.034974	3.571663
173.781906	4310.373946	6.973786	-0.035026	3.574835
174.099575	4318.373811	6.978790	-0.035090	3.578002
174.167878	4326.425249	6.983795	-0.035108	3.581180
174.199050	4334.430298	6.988800	-0.035119	3.584335
174.628120	4342.435751	6.993805	-0.035204	3.587499
174.956229	4350.473252	6.998810	-0.035270	3.590669
175.011086	4358.533769	7.003814	-0.035286	3.593838
175.269781	4366.530274	7.008819	-0.035339	3.596985
175.390891	4374.531843	7.013824	-0.035367	3.600128
175.480493	4382.534752	7.018829	-0.035389	3.603267
175.619906	4390.617699	7.023834	-0.035420	3.606436
175.908790	4398.611760	7.028838	-0.035479	3.609572
176.084405	4406.643329	7.033843	-0.035516	3.612716
176.322009	4414.715175	7.038848	-0.035566	3.615875
176.587163	4422.688998	7.043853	-0.035620	3.618994
176.786645	4430.712903	7.048858	-0.035663	3.622128
176.869917	4438.705515	7.053862	-0.035683	3.625244
176.982445	4446.759974	7.058867	-0.035709	3.628382
177.454053	4454.820472	7.063872	-0.035802	3.631529
177.480997	4462.873340	7.068877	-0.035813	3.634659
177.611478	4470.869653	7.073882	-0.035842	3.637766
178.000876	4478.888753	7.078886	-0.035920	3.640887
178.178324	4486.868304	7.083891	-0.035958	3.643984
178.367676	4494.938608	7.088896	-0.035998	3.647114
178.663674	4502.928683	7.093901	-0.036059	3.650213
179.178796	4510.981785	7.098906	-0.036160	3.653339
179.231120	4519.025111	7.103910	-0.036175	3.656447
179.553686	4526.999433	7.108915	-0.036240	3.659532
179.746223	4535.054277	7.113920	-0.036281	3.662643
179.738945	4543.056619	7.118925	-0.036285	3.665725
180.090613	4551.084472	7.123930	-0.036355	3.668824
180.415426	4559.120272	7.128934	-0.036421	3.671923
180.615778	4567.131536	7.133939	-0.036463	3.675006
180.838753	4575.183907	7.138944	-0.036510	3.678103
180.840150	4583.192820	7.143949	-0.036515	3.681175
181.099982	4591.179007	7.148954	-0.036569	3.684242
181.417015	4599.229348	7.153958	-0.036633	3.687333
181.799983	4607.221822	7.158963	-0.036710	3.690401
182.288319	4615.267279	7.163968	-0.036806	3.693489
182.332912	4623.311265	7.168973	-0.036819	3.696562
182.470870	4631.308383	7.173978	-0.036850	3.699618
182.874635	4639.328384	7.178982	-0.036930	3.702686
183.151000	4647.343854	7.183987	-0.036987	3.705747
183.404695	4655.402832	7.188992	-0.037039	3.708821
183.246829	4663.469008	7.193997	-0.037015	3.711885
183.647370	4671.530367	7.199002	-0.037095	3.714959
183.670287	4679.532435	7.204006	-0.037104	3.717998
183.658327	4687.517790	7.209011	-0.037107	3.721028
184.039260	4695.451549	7.214016	-0.037183	3.724045
184.252173	4703.493334	7.219021	-0.037228	3.727096
184.453387	4711.512849	7.224026	-0.037271	3.730137
184.488995	4719.560243	7.229030	-0.037282	3.733181
184.767423	4727.611272	7.234035	-0.037339	3.736230
184.936768	4735.622942	7.239040	-0.037376	3.739259
184.994697	4743.599347	7.244045	-0.037392	3.742269
185.279335	4751.620201	7.249050	-0.037450	3.745300
185.399375	4759.680354	7.254054	-0.037478	3.748338
185.496970	4767.708669	7.259059	-0.037501	3.751362
185.763406	4775.742998	7.264064	-0.037556	3.754389
185.951220	4783.732276	7.269069	-0.037596	3.757395
186.185866	4791.765917	7.274074	-0.037645	3.760417
186.210329	4799.786581	7.279078	-0.037654	3.763426
186.384616	4807.816165	7.284083	-0.037692	3.766440
186.668585	4815.844729	7.289088	-0.037750	3.769453
186.852662	4823.887601	7.294093	-0.037790	3.772467
187.472026	4831.896369	7.299098	-0.037910	3.775476
187.512392	4839.901698	7.304102	-0.037923	3.778468
187.538293	4847.956937	7.309107	-0.037933	3.781476
187.735935	4855.945485	7.314112	-0.037975	3.784460
188.046670	4863.999015	7.319117	-0.038038	3.787469
187.998931	4872.019285	7.324122	-0.038034	3.790454
188.156483	4880.088196	7.329126	-0.038068	3.793461
188.555037	4888.081245	7.334131	-0.038148	3.796441
188.832772	4896.053438	7.339136	-0.038205	3.799410
188.813532	4904.086517	7.344141	-0.038206	3.802391
188.977714	4912.061238	7.349146	-0.038242	3.805353
188.906290	4920.123457	7.354150	-0.038234	3.808340
189.064473	4928.161713	7.359155	-0.038268	3.811321
189.528449	4936.175888	7.364160	-0.038360	3.814296
189.377878	4944.182333	7.369165	-0.038337	3.817254
189.741692	4952.198167	7.374170	-0.038410	3.820224
189.993547	4960.225161	7.379174	-0.038462	3.823193
190.179483	4968.238590	7.384179	-0.038502	3.826153
190.103454	4976.261436	7.389184	-0.038493	3.829109
190.274717	4984.323840	7.394189	-0.038530	3.832082
190.663133	4992.286909	7.399194	-0.038607	3.835021
190.724833	5000.338451	7.404198	-0.038624	3.837984
190.851894	5008.357715	7.409203	-0.038653	3.840933
191.058494	5016.354068	7.414208	-0.038696	3.843874
191.074161	5024.395428	7.419213	-0.038704	3.846825
191.254949	5032.386053	7.424218	-0.038743	3.849758
191.342838	5040.474129	7.429222	-0.038765	3.852723
191.626892	5048.467169	7.434227	-0.038823	3.855655
192.053273	5056.492710	7.439232	-0.038907	3.858600
192.239845	5064.530086	7.444237	-0.038947	3.861541
192.355300	5072.489504	7.449242	-0.038974	3.864451
192.586206	5080.562481	7.454246	-0.039022	3.867401
193.046399	5088.560726	7.459251	-0.039113	3.870327
193.444975	5096.809416	7.464256	-0.039192	3.873341
193.703967	5104.826085	7.469261	-0.039246	3.876265
193.966987	5112.720806	7.474266	-0.039300	3.879143
194.190781	5120.733571	7.479270	-0.039347	3.882060
194.290955	5128.657636	7.484275	-0.039370	3.884941
194.530036	5136.745413	7.489280	-0.039420	3.887881
194.629651	5144.728013	7.494285	-0.039444	3.890779
194.706427	5152.757457	7.499290	-0.039463	3.893691
194.903719	5160.827126	7.504294	-0.039505	3.896617
195.030745	5168.792736	7.509299	-0.039534	3.899503
195.155896	5176.833491	7.514304	-0.039562	3.902413
195.499941	5184.790252	7.519309	-0.039632	3.905295
195.565504	5192.827186	7.524314	-0.039649	3.908199
195.733076	5200.892549	7.529318	-0.039685	3.911112
195.741959	5208.884703	7.534323	-0.039692	3.913994
196.134626	5216.916790	7.539328	-0.039770	3.916895
196.292812	5224.901944	7.544333	-0.039805	3.919773
196.407474	5232.949082	7.549338	-0.039831	3.922670
196.722498	5240.933846	7.554342	-0.039895	3.925547
196.831792	5248.954140	7.559347	-0.039921	3.928430
197.015443	5257.051456	7.564352	-0.039960	3.931340
197.192443	5265.028072	7.569357	-0.039998	3.934204
197.423304	5273.054071	7.574362	-0.040046	3.937085
197.411471	5281.070237	7.579366	-0.040049	3.939956
197.678284	5289.056615	7.584371	-0.040104	3.942819
198.044925	5297.069309	7.589376	-0.040178	3.945692
198.130472	5305.107957	7.594381	-0.040199	3.948566
198.151389	5313.168792	7.599386	-0.040208	3.951445
198.433314	5321.223653	7.604390	-0.040265	3.954325
198.509718	5329.179778	7.609395	-0.040285	3.957163
198.480007	5337.173088	7.614400	-0.040284	3.960011
198.728241	5345.201712	7.619405	-0.040336	3.962874
199.273536	5353.197405	7.624410	-0.040442	3.965729
199.370608	5361.229332	7.629414	-0.040466	3.968586
199.392381	5369.239920	7.634419	-0.040475	3.971433
199.767920	5377.300173	7.639424	-0.040550	3.974301
199.760883	5385.342248	7.644429	-0.040554	3.977154
199.974989	5393.301292	7.649434	-0.040599	3.979980
200.373760	5401.359688	7.654438	-0.040678	3.982841
200.409572	5409.371311	7.659443	-0.040690	3.985678
200.635617	5417.407186	7.664448	-0.040737	3.988525
200.721077	5425.448346	7.669453	-0.040758	3.991369
200.951804	5433.478864	7.674458	-0.040806	3.994210
201.013808	5441.499946	7.679462	-0.040823	3.997042
201.039016	5449.461150	7.684467	-0.040833	3.999851
201.549568	5457.513960	7.689472	-0.040933	4.002698
201.604246	5465.513596	7.694477	-0.040949	4.005517
201.524684	5473.554233	7.699482	-0.040939	4.008346
201.972181	5481.598149	7.704486	-0.041027	4.011183
202.016720	5489.590464	7.709491	-0.041041	4.013993
202.270666	5497.656428	7.714496	-0.041093	4.016830
202.282481	5505.630401	7.719501	-0.041101	4.019629
202.561641	5513.663135	7.724506	-0.041158	4.022451
202.732242	5521.675223	7.729510	-0.041195	4.025262
202.571872	5529.693210	7.734515	-0.041170	4.028068
202.941391	5537.763233	7.739520	-0.041244	4.030899
203.190547	5545.835384	7.744525	-0.041295	4.033726
203.472247	5553.838639	7.749530	-0.041353	4.036528
203.675754	5561.779411	7.754534	-0.041396	4.039305
203.917422	5569.767947	7.759539	-0.041446	4.042097
204.046490	5577.793772	7.764544	-0.041475	4.044898
204.282961	5585.826044	7.769549	-0.041525	4.047701
204.564999	5593.826203	7.774554	-0.041582	4.050492
204.884013	5601.838526	7.779558	-0.041647	4.053286
204.885728	5609.910190	7.784563	-0.041652	4.056093
205.450000	5617.876886	7.789568	-0.041762	4.058870
205.386269	5625.926547	7.794573	-0.041756	4.061666
205.689064	5633.872149	7.799578	-0.041817	4.064428
205.929580	5641.972603	7.804582	-0.041867	4.067241
206.209638	5649.951021	7.809587	-0.041925	4.070011
206.291581	5658.008867	7.814592	-0.041945	4.072803
206.496668	5665.999636	7.819597	-0.041988	4.075572
206.653770	5674.021337	7.824602	-0.042023	4.078349
206.859702	5682.021325	7.829606	-0.042066	4.081117
206.684654	5690.004056	7.834611	-0.042039	4.083872
206.919580	5698.099789	7.839616	-0.042088	4.086670
207.313049	5706.041012	7.844621	-0.042166	4.089415
207.551408	5714.114323	7.849626	-0.042216	4.092202
207.477772	5722.168272	7.854630	-0.042207	4.094975
207.528738	5730.165659	7.859635	-0.042222	4.097729
207.807090	5738.185980	7.864640	-0.042279	4.100492
207.777063	5746.194639	7.869645	-0.042278	4.103245
207.969403	5754.204697	7.874650	-0.042319	4.106000
208.313396	5762.243548	7.879654	-0.042388	4.108764
208.365272	5770.276285	7.884659	-0.042403	4.111521
208.875150	5778.327221	7.889664	-0.042503	4.114288
208.962849	5786.342219	7.894669	-0.042525	4.117035
209.042375	5794.297249	7.899674	-0.042545	4.119760
209.183689	5802.338345	7.904678	-0.042576	4.122513
209.488014	5810.329541	7.909683	-0.042638	4.125250
209.617025	5818.382886	7.914688	-0.042667	4.128003
209.508857	5826.385408	7.919693	-0.042652	4.130735
209.797171	5834.422697	7.924698	-0.042711	4.133481
209.948031	5842.509808	7.929702	-0.042744	4.136241
209.900955	5850.445482	7.934707	-0.042741	4.138945
210.006688	5858.499154	7.939712	-0.042765	4.141689
210.204145	5866.491640	7.944717	-0.042807	4.144412
210.286047	5874.523861	7.949722	-0.042828	4.147145
210.459361	5882.572905	7.954726	-0.042865	4.149883
210.700797	5890.578988	7.959731	-0.042915	4.152605
210.912237	5898.644837	7.964736	-0.042960	4.155346
210.898626	5906.615263	7.969741	-0.042962	4.158050
211.135890	5914.582241	7.974746	-0.043012	4.160753
211.312221	5922.596231	7.979750	-0.043050	4.163470
211.464145	5930.622822	7.984755	-0.043083	4.166190
211.834485	5938.663952	7.989760	-0.043157	4.168914
211.803273	5946.723088	7.994765	-0.043157	4.171639
211.822869	5954.764530	7.999770	-0.043166	4.174356
212.024612	5962.748754	8.004774	-0.043208	4.177055
212.268655	5970.698888	8.009779	-0.043259	4.179740
212.597071	5978.768154	8.014784	-0.043325	4.182465
212.476679	5986.763892	8.019789	-0.043308	4.185159
212.635602	5994.789050	8.024794	-0.043343	4.187863
212.881548	6002.824082	8.029798	-0.043394	4.190570
212.951273	6010.925781	8.034803	-0.043412	4.193296
213.260028	6018.949910	8.039808	-0.043474	4.195997
213.467730	6026.856107	8.044813	-0.043518	4.198655
213.581927	6034.886636	8.049818	-0.043545	4.201352
213.676801	6042.865270	8.054822	-0.043567	4.204030
213.672322	6050.887524	8.059827	-0.043572	4.206719
213.932604	6058.894614	8.064832	-0.043625	4.209405
214.092620	6066.951982	8.069837	-0.043660	4.212104
214.250606	6074.930659	8.074842	-0.043695	4.214776
214.630867	6083.003917	8.079846	-0.043771	4.217479
214.815486	6090.933292	8.084851	-0.043810	4.220131
214.788422	6099.034907	8.089856	-0.043810	4.222837
214.848648	6107.002509	8.094861	-0.043827	4.225497
215.025719	6115.037248	8.099866	-0.043865	4.228179
214.985991	6123.089155	8.104870	-0.043863	4.230862
215.371325	6131.083144	8.109875	-0.043939	4.233529
215.741338	6139.142819	8.114880	-0.044014	4.236216
215.827470	6147.089218	8.119885	-0.044035	4.238860
216.089650	6155.156754	8.124890	-0.044089	4.241545
216.287516	6163.118559	8.129894	-0.044131	4.244193
216.418986	6171.195447	8.134899	-0.044160	4.246876
216.525427	6179.177512	8.139904	-0.044185	4.249526
216.698148	6187.242807	8.144909	-0.044223	4.252203
216.768400	6195.242596	8.149914	-0.044241	4.254855
217.042642	6203.314417	8.154918	-0.044297	4.257531
217.142458	6211.250898	8.159923	-0.044321	4.260159
217.409576	6219.352062	8.164928	-0.044376	4.262842
217.508037	6227.286330	8.169933	-0.044399	4.265466
217.558199	6235.352526	8.174938	-0.044414	4.268131
217.676285	6243.383220	8.179942	-0.044441	4.270784
217.674400	6251.446716	8.184947	-0.044446	4.273445
218.076933	6259.466831	8.189952	-0.044526	4.276093
218.102781	6267.413706	8.194957	-0.044536	4.278713
218.365369	6275.402058	8.199962	-0.044590	4.281346
218.547237	6283.421216	8.204966	-0.044629	4.283987
218.808084	6291.472838	8.209971	-0.044682	4.286638
219.271672	6299.481726	8.214976	-0.044774	4.289275
219.273056	6307.516743	8.219981	-0.044779	4.291915
219.270279	6315.513068	8.224986	-0.044784	4.294540
219.713110	6323.576658	8.229990	-0.044872	4.297190
219.917853	6331.527401	8.234995	-0.044915	4.299799
219.920881	6339.571776	8.240000	-0.044921	4.302436
220.055697	6347.575991	8.245005	-0.044951	4.305058
220.357541	6355.561154	8.250010	-0.045012	4.307675
220.447608	6363.655561	8.255014	-0.045034	4.310323
220.210637	6371.631756	8.260019	-0.044995	4.312929
220.606329	6379.705101	8.265024	-0.045074	4.315570
220.737214	6387.679649	8.270029	-0.045103	4.318175
220.897851	6395.671794	8.275034	-0.045139	4.320785
221.133849	6403.704486	8.280038	-0.045188	4.323406
221.298317	6411.702555	8.285043	-0.045223	4.326014
221.288420	6419.741985	8.290048	-0.045227	4.328633
221.540168	6427.766150	8.295053	-0.045279	4.331247
221.860523	6435.754424	8.300058	-0.045344	4.333848
222.139594	6443.838807	8.305062	-0.045401	4.336479
222.090318	6451.804536	8.310067	-0.045397	4.339067
222.471785	6459.847622	8.315072	-0.045473	4.341682
222.385771	6467.770819	8.320077	-0.045462	4.344253
222.589944	6475.854396	8.325082	-0.045505	4.346876
222.739741	6483.874703	8.330086	-0.045538	4.349477
223.037084	6491.918076	8.335091	-0.045599	4.352085
223.154167	6500.033702	8.340096	-0.045626	4.354713
223.121790	6507.969079	8.345101	-0.045625	4.357281
223.365824	6515.906550	8.350106	-0.045675	4.359849
223.439841	6523.975823	8.355110	-0.045694	4.362458
223.364656	6531.926207	8.360115	-0.045685	4.365025
223.957882	6539.969969	8.365120	-0.045801	4.367626
224.122985	6547.943674	8.370125	-0.045837	4.370199
224.067374	6556.012516	8.375130	-0.045832	4.372800
224.205079	6564.067035	8.380134	-0.045862	4.375397
224.413350	6571.990306	8.385139	-0.045906	4.377949
224.481799	6580.063480	8.390144	-0.045924	4.380548
224.680474	6588.071168	8.395149	-0.045966	4.383125
224.944347	6596.059175	8.400154	-0.046021	4.385695
225.011511	6604.095310	8.405158	-0.046038	4.388277
225.050630	6612.097799	8.410163	-0.046051	4.390846
225.550245	6620.172945	8.415168	-0.046149	4.393441
225.468389	6628.210428	8.420173	-0.046139	4.396018
225.443016	6636.202932	8.425178	-0.046139	4.398579
225.566538	6644.245374	8.430182	-0.046168	4.401156
225.848531	6652.175839	8.435187	-0.046225	4.403697
225.821171	6660.227321	8.440192	-0.046225	4.406273
225.967118	6668.239697	8.445197	-0.046258	4.408835
226.210726	6676.254269	8.450202	-0.046308	4.411398
226.432250	6684.313064	8.455206	-0.046354	4.413973
226.385906	6692.346581	8.460211	-0.046351	4.416537
226.382383	6700.361584	8.465216	-0.046355	4.419094
226.570617	6708.388124	8.470221	-0.046396	4.421654
226.854951	6716.338577	8.475226	-0.046454	4.424189
227.158013	6724.387573	8.480230	-0.046515	4.426754
227.244598	6732.414101	8.485235	-0.046537	4.429309
227.453429	6740.469075	8.490240	-0.046581	4.431872
227.595011	6748.478674	8.495245	-0.046612	4.434419
227.948963	6756.516512	8.500250	-0.046683	4.436974
228.202404	6764.498558	8.505254	-0.046736	4.439510
228.107688	6772.490006	8.510259	-0.046723	4.442045
228.277713	6780.479491	8.515264	-0.046760	4.444580
228.482483	6788.527337	8.520269	-0.046803	4.447132
228.529210	6796.526748	8.525274	-0.046817	4.449667
228.776026	6804.582430	8.530278	-0.046868	4.452218
229.116205	6812.603173	8.535283	-0.046937	4.454758
229.420460	6820.633031	8.540288	-0.046998	4.457298
229.266886	6828.606998	8.545293	-0.046975	4.459818
229.489849	6836.621423	8.550298	-0.047022	4.462351
229.850836	6844.610177	8.555302	-0.047094	4.464874
229.871012	6852.643199	8.560307	-0.047103	4.467409
229.909710	6860.683558	8.565312	-0.047115	4.469945
230.006621	6868.709024	8.570317	-0.047138	4.472474
230.096108	6876.722308	8.575322	-0.047160	4.474999
230.245834	6884.755376	8.580327	-0.047193	4.477528
230.418488	6892.697526	8.585331	-0.047231	4.480028
230.622259	6900.746149	8.590336	-0.047274	4.482559
230.623000	6908.718030	8.595341	-0.047279	4.485065
230.836705	6916.787673	8.600346	-0.047324	4.487600
230.922353	6924.797583	8.605351	-0.047345	4.490115
231.181640	6932.823280	8.610355	-0.047398	4.492634
231.385690	6940.852125	8.615360	-0.047442	4.495152
231.309607	6948.849305	8.620365	-0.047433	4.497658
231.448092	6956.837999	8.625370	-0.047463	4.500161
231.545122	6964.889433	8.630375	-0.047487	4.502681
231.977430	6972.845677	8.635379	-0.047572	4.505172
232.062091	6980.905344	8.640384	-0.047593	4.507692
231.935244	6988.945345	8.645389	-0.047575	4.510204
232.095260	6997.002448	8.650394	-0.047610	4.512721
232.514612	7005.030047	8.655399	-0.047693	4.515228
232.625670	7012.995603	8.660403	-0.047719	4.517714
232.662133	7020.971169	8.665408	-0.047731	4.520201
232.918738	7028.999630	8.670413	-0.047784	4.522703
233.013580	7036.957607	8.675418	-0.047806	4.525182
233.052965	7045.048787	8.680423	-0.047819	4.527701
233.093648	7053.016007	8.685427	-0.047832	4.530180
233.464298	7061.080849	8.690432	-0.047906	4.532688
233.428318	7069.102669	8.695437	-0.047904	4.535181
233.491785	7077.102139	8.700442	-0.047921	4.537666
233.675956	7085.077134	8.705447	-0.047961	4.540142
233.891963	7093.095632	8.710451	-0.048006	4.542630
234.144423	7101.103307	8.715456	-0.048058	4.545114
234.222067	7109.161760	8.720461	-0.048078	4.547612
234.290711	7117.142057	8.725466	-0.048096	4.550084
234.448143	7125.241278	8.730471	-0.048130	4.552591
234.509131	7133.223374	8.735475	-0.048147	4.555061
235.013979	7141.233022	8.740480	-0.048246	4.557539
234.969338	7149.236540	8.745485	-0.048243	4.560012
235.020400	7157.239943	8.750490	-0.048257	4.562484
235.411475	7165.218013	8.755495	-0.048335	4.564948
235.455517	7173.258569	8.760499	-0.048349	4.567429
235.465224	7181.310736	8.765504	-0.048356	4.569912
235.789935	7189.334793	8.770509	-0.048421	4.572386
235.814547	7197.312612	8.775514	-0.048431	4.574844
235.912550	7205.370583	8.780519	-0.048454	4.577325
236.098023	7213.362696	8.785523	-0.048494	4.579784
236.324328	7221.440306	8.790528	-0.048541	4.582269
236.533699	7229.393415	8.795533	-0.048585	4.584713
236.598206	7237.403032	8.800538	-0.048603	4.587174
236.770767	7245.423874	8.805543	-0.048640	4.589637
236.837570	7253.458459	8.810547	-0.048658	4.592103
236.965009	7261.526819	8.815552	-0.048686	4.594578
236.968624	7269.545785	8.820557	-0.048692	4.597036
237.442316	7277.489947	8.825562	-0.048786	4.599470
237.596970	7285.574501	8.830567	-0.048820	4.601946
237.476460	7293.472934	8.835571	-0.048802	4.604363
237.660963	7301.570237	8.840576	-0.048842	4.606840
237.821066	7309.557591	8.845581	-0.048877	4.609282
237.728190	7317.614747	8.850586	-0.048865	4.611744
238.011030	7325.617836	8.855591	-0.048922	4.614189
238.196161	7333.647791	8.860595	-0.048962	4.616640
238.326216	7341.612474	8.865600	-0.048991	4.619070
238.544912	7349.685911	8.870605	-0.049037	4.621531
238.693763	7357.639712	8.875610	-0.049070	4.623955
239.085414	7365.714829	8.880615	-0.049148	4.626415
239.173214	7373.693567	8.885619	-0.049170	4.628844
239.205283	7381.726762	8.890624	-0.049181	4.631288
239.340453	7389.786957	8.895629	-0.049211	4.633739
239.484752	7397.783683	8.900634	-0.049243	4.636169
239.701709	7405.777603	8.905639	-0.049289	4.638598
239.979597	7413.781067	8.910643	-0.049346	4.641028
240.146615	7421.798890	8.915648	-0.049382	4.643460
240.237084	7429.808454	8.920653	-0.049404	4.645890
240.236075	7437.808626	8.925658	-0.049409	4.648315
240.440193	7445.863023	8.930663	-0.049452	4.650755
240.507341	7453.873895	8.935667	-0.049470	4.653181
240.837627	7461.891873	8.940672	-0.049536	4.655607
240.932391	7469.879315	8.945677	-0.049559	4.658023
240.870586	7477.876592	8.950682	-0.049553	4.660441
241.120496	7485.931873	8.955687	-0.049604	4.662875
241.412418	7493.862388	8.960691	-0.049664	4.665270
241.541609	7501.969188	8.965696	-0.049693	4.667717
241.601101	7509.974425	8.970701	-0.049709	4.670132
241.714187	7518.019289	8.975706	-0.049736	4.672558
241.998508	7526.085769	8.980711	-0.049794	4.674989
242.076007	7534.080910	8.985715	-0.049813	4.677397
242.485013	7542.003073	8.990720	-0.049894	4.679782
242.591325	7550.059632	8.995725	-0.049919	4.682206
242.721349	7558.003220	9.000730	-0.049949	4.684595
242.909030	7566.090449	9.005735	-0.049989	4.687026
242.975785	7573.988964	9.010739	-0.050006	4.689399
243.047117	7582.099520	9.015744	-0.050025	4.691834
243.246849	7590.149582	9.020749	-0.050067	4.694250
243.396090	7598.163993	9.025754	-0.050100	4.696654
243.560626	7606.127477	9.030759	-0.050136	4.699042
243.527877	7614.116655	9.035763	-0.050135	4.701436
243.848730	7622.105093	9.040768	-0.050200	4.703828
244.146881	7630.149720	9.045773	-0.050261	4.706236
244.195824	7638.167515	9.050778	-0.050275	4.708634
244.293982	7646.248276	9.055783	-0.050298	4.711051
244.772189	7654.249492	9.060787	-0.050392	4.713441
244.781378	7662.300329	9.065792	-0.050399	4.715847
244.745939	7670.279622	9.070797	-0.050398	4.718229
244.966908	7678.272423	9.075802	-0.050444	4.720614
245.415415	7686.271316	9.080807	-0.050533	4.722999
245.364183	7694.286794	9.085811	-0.050528	4.725389
245.568116	7702.311757	9.090816	-0.050571	4.727780
245.580797	7710.360080	9.095821	-0.050579	4.730177
245.657577	7718.403659	9.100826	-0.050598	4.732571
245.761820	7726.407531	9.105831	-0.050623	4.734952
246.013804	7734.438974	9.110835	-0.050675	4.737340
246.322415	7742.399495	9.115840	-0.050738	4.739705
246.323051	7750.446130	9.120845	-0.050743	4.742096
246.562415	7758.400449	9.125850	-0.050793	4.744457
246.957946	7766.475168	9.130855	-0.050871	4.746852
246.905587	7774.460882	9.135859	-0.050867	4.749221
247.042017	7782.512672	9.140864	-0.050897	4.751608
247.027692	7790.597453	9.145869	-0.050900	4.754004
247.151091	7798.569789	9.150874	-0.050928	4.756365
247.260251	7806.523824	9.155879	-0.050954	4.758719
247.427432	7814.577514	9.160883	-0.050990	4.761101
247.771256	7822.529708	9.165888	-0.051059	4.763452
247.907547	7830.569030	9.170893	-0.051089	4.765828
247.871483	7838.524686	9.175898	-0.051088	4.768178
248.108596	7846.628326	9.180903	-0.051137	4.770570
248.015041	7854.625072	9.185907	-0.051125	4.772931
248.184348	7862.624902	9.190912	-0.051162	4.775290
248.575530	7870.699446	9.195917	-0.051240	4.777669
248.534134	7878.636796	9.200922	-0.051237	4.780009
248.625844	7886.733542	9.205927	-0.051259	4.782393
248.868377	7894.650813	9.210931	-0.051310	4.784723
249.107603	7902.719505	9.215936	-0.051359	4.787097
249.170994	7910.755854	9.220941	-0.051376	4.789460
249.401204	7918.758215	9.225946	-0.051424	4.791812
249.717574	7926.799857	9.230951	-0.051488	4.794173
249.584575	7934.763517	9.235955	-0.051469	4.796512
249.701303	7942.770897	9.240960	-0.051496	4.798862
250.037584	7950.797262	9.245965	-0.051563	4.801216
250.019896	7958.742445	9.250970	-0.051565	4.803546
250.127163	7966.810610	9.255975	-0.051590	4.805910
250.222979	7974.857035	9.260979	-0.051613	4.808267
250.576150	7982.893390	9.265984	-0.051684	4.810618
250.585019	7990.309454	9.270989	-0.051691	4.812789
250.629115	7994.921202	9.275994	-0.051702	4.814138

250.972191	7997.518291	9.280999	-0.051767	4.814896
250.938207	7998.884131	9.286003	-0.051762	4.815295
251.025666	7999.317902	9.291008	-0.051778	4.815422
251.063522	8000.240917	9.296013	-0.051786	4.815691
251.277449	8000.237977	9.301018	-0.051826	4.815690
251.403883	8000.277391	9.306023	-0.051849	4.815700
251.343679	8000.242242	9.311027	-0.051838	4.815690
251.530665	8000.271963	9.316032	-0.051873	4.815698
251.464106	8000.263402	9.321037	-0.051860	4.815696
251.206161	8000.242126	9.326042	-0.051812	4.815691
251.625378	8000.269211	9.331047	-0.051890	4.815697
251.465832	8000.263411	9.336051	-0.051860	4.815696
251.632485	8000.301342	9.341056	-0.051891	4.815706
251.837116	8000.274764	9.346061	-0.051929	4.815698
251.803030	8000.262460	9.351066	-0.051923	4.815694
251.779813	8000.303715	9.356071	-0.051918	4.815706
251.807413	8000.272127	9.361075	-0.051923	4.815697
252.053750	8000.291068	9.366080	-0.051969	4.815701
251.891374	8000.240380	9.371085	-0.051939	4.815687
251.934884	8000.274178	9.376090	-0.051947	4.815697
252.111612	8000.293056	9.381095	-0.051980	4.815702
252.174664	8000.274856	9.386099	-0.051991	4.815696
251.952634	8000.246687	9.391104	-0.051950	4.815689
251.934734	8000.243187	9.396109	-0.051947	4.815688
252.031446	8000.249022	9.401114	-0.051965	4.815689
252.216879	8000.280854	9.406119	-0.051999	4.815698
252.085378	8000.256291	9.411123	-0.051974	4.815691
252.198425	8000.325383	9.416128	-0.051995	4.815711
252.179601	8000.294108	9.421133	-0.051992	4.815702
252.253940	8000.269685	9.426138	-0.052006	4.815694
252.517249	8000.289971	9.431143	-0.052055	4.815699
252.193179	8000.261212	9.436147	-0.051994	4.815692
252.220566	8000.283003	9.441152	-0.051999	4.815698
252.316301	8000.261063	9.446157	-0.052017	4.815691
252.385124	8000.278189	9.451162	-0.052030	4.815696
252.461289	8000.293300	9.456167	-0.052044	4.815700
252.466398	8000.258143	9.461171	-0.052045	4.815690
252.647100	8000.286696	9.466176	-0.052078	4.815697
252.701290	8000.248066	9.471181	-0.052088	4.815686
252.523485	8000.279337	9.476186	-0.052055	4.815696
252.755380	8000.330075	9.481191	-0.052098	4.815710
252.712320	8000.292000	9.486195	-0.052090	4.815699
252.751952	8000.295840	9.491200	-0.052097	4.815700
252.514272	8000.293041	9.496205	-0.052053	4.815700
252.624489	8000.294824	9.501210	-0.052073	4.815700
252.668407	8000.309411	9.506215	-0.052082	4.815704
252.559810	8000.290558	9.511219	-0.052061	4.815699
252.621679	8000.318248	9.516224	-0.052073	4.815707
252.668276	8000.278427	9.521229	-0.052081	4.815695
252.521694	8000.273904	9.526234	-0.052054	4.815694
252.870393	8000.298780	9.531239	-0.052119	4.815700
252.708893	8000.282270	9.536243	-0.052089	4.815696
252.784542	8000.302711	9.541248	-0.052103	4.815701
252.909808	8000.301536	9.546253	-0.052126	4.815700
252.898169	8000.290664	9.551258	-0.052124	4.815697
252.950739	8000.288308	9.556263	-0.052133	4.815696
252.715791	8000.260996	9.561267	-0.052090	4.815690
253.031081	8000.302413	9.566272	-0.052148	4.815700
252.999971	8000.293359	9.571277	-0.052142	4.815698
252.915703	8000.299458	9.576282	-0.052127	4.815700
253.011034	8000.310609	9.581287	-0.052144	4.815703
252.821975	8000.271230	9.586291	-0.052109	4.815692
252.799221	8000.299681	9.591296	-0.052105	4.815700
252.810119	8000.287040	9.596301	-0.052107	4.815697
252.820026	8000.280788	9.601306	-0.052108	4.815695
253.145963	8000.311701	9.606311	-0.052169	4.815702
253.081422	8000.288225	9.611315	-0.052157	4.815696
253.060116	8000.299617	9.616320	-0.052153	4.815699
253.184787	8000.281350	9.621325	-0.052176	4.815693
252.924825	8000.289932	9.626330	-0.052128	4.815697
252.985273	8000.312261	9.631335	-0.052139	4.815703
253.029324	8000.273466	9.636339	-0.052147	4.815692
253.152992	8000.294687	9.641344	-0.052170	4.815697
253.127952	8000.317763	9.646349	-0.052165	4.815704
253.101479	8000.308784	9.651354	-0.052160	4.815702
253.214518	8000.312750	9.656359	-0.052181	4.815702
253.049602	8000.321809	9.661363	-0.052150	4.815706
253.079755	8000.354323	9.666368	-0.052156	4.815715
253.067730	8000.311413	9.671373	-0.052153	4.815703
252.972946	8000.283175	9.676378	-0.052136	4.815695
253.056275	8000.340042	9.681383	-0.052151	4.815711
252.982621	8000.300402	9.686387	-0.052137	4.815700
253.064928	8000.334831	9.691392	-0.052153	4.815710
253.058154	8000.311225	9.696397	-0.052151	4.815703
253.066620	8000.334845	9.701402	-0.052153	4.815710
253.125211	8000.311234	9.706407	-0.052164	4.815702
253.068985	8000.284689	9.711411	-0.052153	4.815695
253.096533	8000.342786	9.716416	-0.052158	4.815712
253.306336	8000.313090	9.721421	-0.052197	4.815702
253.150536	8000.337244	9.726426	-0.052168	4.815710
253.031697	8000.348119	9.731431	-0.052146	4.815714
253.148160	8000.287011	9.736435	-0.052167	4.815695
253.216976	8000.298799	9.741440	-0.052180	4.815698
253.241911	8000.302401	9.746445	-0.052185	4.815699
253.323964	8000.312269	9.751450	-0.052200	4.815702
253.591314	8000.337961	9.756455	-0.052250	4.815708
253.230325	8000.280840	9.761459	-0.052182	4.815693
253.218896	8000.314813	9.766464	-0.052180	4.815703
253.355606	8000.314893	9.771469	-0.052206	4.815702
253.347347	8000.304075	9.776474	-0.052204	4.815699
253.186536	8000.330283	9.781479	-0.052174	4.815708
253.042274	8000.299105	9.786483	-0.052147	4.815699
253.375577	8000.344019	9.791488	-0.052209	4.815711
253.401991	8000.336968	9.796493	-0.052214	4.815709
253.289801	8000.311649	9.801498	-0.052193	4.815702
253.527350	8000.303758	9.806503	-0.052237	4.815698
253.248410	8000.292813	9.811507	-0.052185	4.815696
253.200934	8000.311253	9.816512	-0.052176	4.815702
253.245256	8000.315170	9.821517	-0.052184	4.815703
253.265783	8000.275993	9.826522	-0.052188	4.815691
253.366237	8000.312852	9.831527	-0.052207	4.815702
253.413073	8000.309336	9.836531	-0.052215	4.815700
253.676595	8000.321086	9.841536	-0.052264	4.815703
253.470729	8000.330546	9.846541	-0.052226	4.815706
253.354673	8000.309435	9.851546	-0.052204	4.815701
253.512640	8000.314131	9.856551	-0.052234	4.815701
253.566460	8000.284036	9.861555	-0.052243	4.815692
253.361302	8000.330877	9.866560	-0.052205	4.815707
253.423542	8000.372455	9.871565	-0.052217	4.815719
253.585678	8000.323833	9.876570	-0.052247	4.815704
253.518386	8000.345155	9.881575	-0.052234	4.815710
253.499378	8000.298929	9.886579	-0.052231	4.815697
253.557977	8000.310551	9.891584	-0.052241	4.815700
253.561098	8000.304189	9.896589	-0.052242	4.815698
253.446659	8000.292714	9.901594	-0.052221	4.815695
253.595619	8000.355987	9.906599	-0.052248	4.815713
253.604417	8000.307009	9.911603	-0.052250	4.815699
253.538222	8000.329416	9.916608	-0.052237	4.815706
253.595417	8000.307918	9.921613	-0.052248	4.815699
253.626920	8000.291340	9.926618	-0.052254	4.815694
253.670793	8000.333687	9.931623	-0.052262	4.815706
253.636123	8000.271190	9.936627	-0.052255	4.815688
253.656067	8000.301403	9.941632	-0.052259	4.815697
253.497292	8000.292410	9.946637	-0.052229	4.815695
253.463734	8000.286520	9.951642	-0.052223	4.815694
253.617618	8000.319978	9.956647	-0.052252	4.815703
253.618797	8000.307178	9.961651	-0.052252	4.815699
253.625268	8000.324360	9.966656	-0.052253	4.815704
253.719576	8000.283178	9.971661	-0.052270	4.815691
253.836295	8000.298948	9.976666	-0.052292	4.815695
253.713289	8000.332177	9.981671	-0.052269	4.815706
253.437149	8000.299923	9.986675	-0.052218	4.815698
253.681562	8000.329513	9.991680	-0.052263	4.815705
253.566124	8000.326563	9.996685	-0.052241	4.815705
253.620789	8000.316767	10.001690	-0.052252	4.815702
253.765991	8000.360761	10.006695	-0.052279	4.815714
253.566524	8000.285977	10.011699	-0.052241	4.815693
253.703736	8000.329841	10.016704	-0.052267	4.815705
253.764996	8000.329762	10.021709	-0.052278	4.815705
253.691940	8000.321094	10.026714	-0.052264	4.815703
253.639562	8000.310627	10.031719	-0.052255	4.815700
253.619308	8000.306021	10.036723	-0.052251	4.815699
253.636523	8000.299888	10.041728	-0.052254	4.815697
253.773540	8000.317056	10.046733	-0.052279	4.815701
253.738594	8000.326091	10.051738	-0.052273	4.815704
253.802309	8000.335661	10.056743	-0.052285	4.815706
253.877426	8000.290964	10.061747	-0.052298	4.815693
253.747662	8000.324083	10.066752	-0.052274	4.815703
253.829452	8000.274156	10.071757	-0.052289	4.815688
253.715096	8000.291510	10.076762	-0.052268	4.815694
253.800697	8000.372972	10.081767	-0.052284	4.815717
253.543889	8000.341032	10.086771	-0.052236	4.815709
253.706119	8000.355407	10.091776	-0.052266	4.815713
253.921169	8000.323661	10.096781	-0.052306	4.815702
253.835939	8000.320134	10.101786	-0.052290	4.815702
253.703870	8000.360689	10.106791	-0.052265	4.815714
253.828395	8000.316795	10.111795	-0.052289	4.815701
253.988379	8000.351420	10.116800	-0.052318	4.815710
253.913756	8000.334185	10.121805	-0.052304	4.815705
253.961198	8000.314663	10.126810	-0.052313	4.815700
253.946146	8000.328292	10.131815	-0.052310	4.815704
253.740793	8000.311068	10.136819	-0.052272	4.815700
253.805582	8000.335604	10.141824	-0.052284	4.815706
253.840996	8000.309480	10.146829	-0.052290	4.815699
253.792386	8000.292668	10.151834	-0.052281	4.815694
253.906324	8000.309461	10.156839	-0.052302	4.815698
253.820997	8000.288849	10.161843	-0.052286	4.815693
253.985779	8000.307537	10.166848	-0.052317	4.815697
253.856521	8000.301159	10.171853	-0.052293	4.815696
253.762781	8000.311373	10.176858	-0.052275	4.815700
253.883208	8000.330407	10.181863	-0.052298	4.815705
253.989159	8000.323581	10.186867	-0.052317	4.815702
253.977045	8000.306294	10.191872	-0.052315	4.815697
254.076769	8000.304706	10.196877	-0.052334	4.815696
253.694086	8000.300615	10.201882	-0.052262	4.815697
253.959154	8000.357234	10.206887	-0.052312	4.815712
253.936085	8000.303467	10.211891	-0.052307	4.815696
253.845860	8000.312671	10.216896	-0.052290	4.815700
253.793421	8000.281917	10.221901	-0.052280	4.815691
253.819454	8000.301552	10.226906	-0.052285	4.815696
254.044380	8000.322285	10.231911	-0.052327	4.815701
253.831819	8000.298537	10.236915	-0.052287	4.815695
253.867499	8000.331142	10.241920	-0.052294	4.815705
253.820296	8000.316488	10.246925	-0.052285	4.815701
253.983641	8000.311662	10.251930	-0.052315	4.815699
253.816251	8000.323883	10.256935	-0.052284	4.815703
253.851733	8000.300964	10.261939	-0.052291	4.815696
254.080518	8000.319623	10.266944	-0.052333	4.815700
253.873013	8000.318380	10.271949	-0.052294	4.815701
253.758937	8000.293030	10.276954	-0.052273	4.815694
253.838231	8000.319937	10.281959	-0.052288	4.815702
253.958040	8000.298388	10.286963	-0.052310	4.815695
253.895673	8000.312316	10.291968	-0.052298	4.815699
253.926040	8000.321344	10.296973	-0.052304	4.815702
253.954542	8000.279093	10.301978	-0.052309	4.815689
253.931470	8000.331029	10.306983	-0.052305	4.815705
253.992640	8000.304256	10.311987	-0.052316	4.815696
254.146457	8000.327036	10.316992	-0.052345	4.815702
254.136143	8000.326862	10.321997	-0.052343	4.815702
253.821062	8000.312125	10.327002	-0.052284	4.815700
254.098113	8000.305945	10.332007	-0.052335	4.815696
254.017228	8000.288608	10.337011	-0.052320	4.815692
254.078334	8000.294933	10.342016	-0.052332	4.815693
254.227821	8000.312304	10.347021	-0.052359	4.815698
254.131361	8000.298985	10.352026	-0.052341	4.815694
253.913770	8000.334947	10.357031	-0.052301	4.815706
254.054163	8000.293446	10.362035	-0.052327	4.815693
253.925001	8000.319101	10.367040	-0.052303	4.815701
254.075730	8000.303393	10.372045	-0.052331	4.815696
254.077504	8000.300212	10.377050	-0.052331	4.815695
254.274939	8000.331176	10.382055	-0.052368	4.815703
253.942393	8000.306545	10.387059	-0.052306	4.815697
253.849401	8000.290079	10.392064	-0.052288	4.815693
253.970027	8000.297372	10.397069	-0.052311	4.815695
253.982403	8000.289025	10.402074	-0.052313	4.815692
253.935421	8000.323489	10.407079	-0.052304	4.815702
253.909026	8000.307038	10.412083	-0.052299	4.815698
254.091398	8000.322808	10.417088	-0.052333	4.815701
254.188060	8000.282732	10.422093	-0.052351	4.815689
253.879660	8000.297999	10.427098	-0.052293	4.815695
254.079486	8000.326866	10.432103	-0.052331	4.815703
254.051919	8000.293312	10.437107	-0.052325	4.815693
254.022119	8000.291754	10.442112	-0.052320	4.815693
254.145791	8000.311908	10.447117	-0.052343	4.815698
254.021505	8000.291731	10.452122	-0.052319	4.815693
253.955504	8000.310938	10.457127	-0.052307	4.815699
253.968547	8000.262029	10.462131	-0.052309	4.815684
254.148710	8000.287372	10.467136	-0.052343	4.815691
253.793335	8000.287996	10.472141	-0.052277	4.815693
253.891528	8000.282112	10.477146	-0.052295	4.815690
254.131881	8000.319111	10.482151	-0.052340	4.815700
254.196864	8000.303077	10.487155	-0.052352	4.815695
254.037412	8000.330375	10.492160	-0.052322	4.815704
254.163205	8000.320668	10.497165	-0.052345	4.815700
254.152715	8000.280986	10.502170	-0.052343	4.815689
254.187831	8000.332800	10.507175	-0.052350	4.815704
253.994921	8000.308304	10.512179	-0.052314	4.815698
254.029464	8000.299249	10.517184	-0.052320	4.815695
254.140527	8000.298913	10.522189	-0.052341	4.815694
254.219728	8000.307667	10.527194	-0.052355	4.815696
254.309583	8000.326205	10.532199	-0.052372	4.815701
254.230095	8000.291807	10.537203	-0.052357	4.815692
254.094459	8000.318424	10.542208	-0.052332	4.815700
254.135442	8000.310542	10.547213	-0.052339	4.815698
254.208064	8000.312784	10.552218	-0.052353	4.815698
254.418394	8000.319399	10.557223	-0.052392	4.815699
254.372887	8000.299434	10.562227	-0.052383	4.815693
254.361009	8000.297099	10.567232	-0.052381	4.815693
254.342854	8000.321355	10.572237	-0.052377	4.815700
254.051396	8000.316611	10.577242	-0.052323	4.815700
254.409185	8000.356587	10.582247	-0.052390	4.815710
254.426658	8000.306682	10.587251	-0.052393	4.815695
254.236043	8000.315322	10.592256	-0.052357	4.815699
254.145836	8000.334136	10.597261	-0.052340	4.815705
254.108117	8000.312162	10.602266	-0.052333	4.815698
254.255983	8000.306017	10.607271	-0.052361	4.815696
254.110755	8000.303650	10.612275	-0.052334	4.815696
254.349835	8000.307530	10.617280	-0.052378	4.815696
254.459499	8000.325322	10.622285	-0.052398	4.815700
254.209525	8000.309507	10.627290	-0.052352	4.815697
254.089772	8000.326772	10.632295	-0.052329	4.815703
254.120097	8000.280280	10.637299	-0.052335	4.815689
254.153663	8000.303241	10.642304	-0.052341	4.815695
254.242541	8000.316424	10.647309	-0.052358	4.815699
254.181117	8000.292997	10.652314	-0.052346	4.815692
254.204343	8000.343550	10.657319	-0.052350	4.815707
254.186907	8000.304823	10.662323	-0.052347	4.815696
254.182645	8000.319695	10.667328	-0.052346	4.815700
254.260360	8000.318816	10.672333	-0.052361	4.815700
254.102265	8000.257516	10.677338	-0.052331	4.815682
254.368688	8000.323767	10.682343	-0.052381	4.815700
254.620121	8000.301155	10.687347	-0.052427	4.815693
254.424648	8000.312919	10.692352	-0.052391	4.815697
254.255170	8000.315496	10.697357	-0.052359	4.815699
254.354186	8000.313896	10.702362	-0.052378	4.815698
254.389998	8000.331555	10.707367	-0.052384	4.815703
254.270570	8000.300779	10.712371	-0.052362	4.815694
254.232611	8000.324713	10.717376	-0.052355	4.815701
254.378764	8000.336692	10.722381	-0.052382	4.815704
254.378977	8000.292912	10.727386	-0.052382	4.815691
254.224550	8000.298937	10.732391	-0.052353	4.815694
254.240224	8000.284237	10.737395	-0.052356	4.815690
254.319043	8000.319679	10.742400	-0.052371	4.815700
254.511122	8000.323863	10.747405	-0.052406	4.815700
254.385138	8000.302589	10.752410	-0.052383	4.815694
254.334294	8000.332720	10.757415	-0.052373	4.815703
254.280886	8000.301949	10.762419	-0.052363	4.815695
254.321345	8000.331429	10.767424	-0.052371	4.815703
254.361198	8000.317122	10.772429	-0.052378	4.815699
254.282454	8000.331851	10.777434	-0.052363	4.815703
254.261078	8000.326159	10.782439	-0.052359	4.815702
254.554909	8000.330929	10.787443	-0.052414	4.815702
254.608995	8000.329666	10.792448	-0.052424	4.815701
254.518616	8000.307904	10.797453	-0.052407	4.815695
254.391089	8000.285537	10.802458	-0.052383	4.815689
254.349968	8000.322232	10.807463	-0.052375	4.815700
254.212730	8000.290099	10.812467	-0.052350	4.815691
254.188791	8000.313193	10.817472	-0.052345	4.815698
254.464471	8000.316600	10.822477	-0.052396	4.815698
254.268010	8000.288843	10.827482	-0.052360	4.815691
254.353741	8000.317990	10.832487	-0.052376	4.815699
254.265043	8000.302662	10.837491	-0.052359	4.815695
254.349475	8000.306163	10.842496	-0.052375	4.815695
254.260421	8000.324996	10.847501	-0.052358	4.815701
254.298549	8000.309593	10.852506	-0.052365	4.815697
254.237155	8000.329943	10.857511	-0.052354	4.815703
254.224337	8000.289155	10.862515	-0.052351	4.815691
254.323870	8000.312121	10.867520	-0.052370	4.815697
254.623450	8000.276411	10.872525	-0.052425	4.815685
254.491875	8000.273198	10.877530	-0.052401	4.815685
254.510411	8000.331149	10.882535	-0.052404	4.815702
254.433007	8000.270092	10.887539	-0.052390	4.815685
254.427633	8000.318046	10.892544	-0.052388	4.815699
254.383701	8000.304512	10.897549	-0.052380	4.815695
254.421174	8000.296573	10.902554	-0.052387	4.815692
254.596296	8000.280195	10.907559	-0.052420	4.815687
254.609492	8000.269726	10.912563	-0.052422	4.815684
254.503459	8000.296824	10.917568	-0.052402	4.815692
254.578726	8000.299108	10.922573	-0.052416	4.815692
254.331986	8000.310039	10.927578	-0.052370	4.815697
254.446485	8000.338587	10.932583	-0.052391	4.815705
254.353789	8000.305042	10.937587	-0.052374	4.815695
254.333551	8000.333535	10.942592	-0.052370	4.815704
254.378912	8000.332130	10.947597	-0.052379	4.815703
254.246027	8000.306474	10.952602	-0.052354	4.815696
254.670169	8000.341123	10.957607	-0.052433	4.815704
254.500242	8000.299916	10.962611	-0.052401	4.815693
254.273744	8000.320785	10.967616	-0.052359	4.815700
254.321250	8000.313009	10.972621	-0.052367	4.815698
254.600460	8000.303661	10.977626	-0.052419	4.815694
254.442725	8000.319241	10.982631	-0.052390	4.815699
254.553800	8000.278332	10.987635	-0.052411	4.815686
254.448938	8000.307585	10.992640	-0.052391	4.815695
254.329641	8000.321655	10.997645	-0.052369	4.815700
254.274527	8000.299398	11.002650	-0.052358	4.815694
254.356624	8000.326351	11.007655	-0.052374	4.815701
254.526724	8000.292807	11.012659	-0.052405	4.815691
254.363084	8000.289073	11.017664	-0.052375	4.815690
254.410328	8000.288767	11.022669	-0.052383	4.815690
254.401949	8000.282218	11.027674	-0.052382	4.815688
254.354758	8000.324153	11.032679	-0.052373	4.815701
254.232355	8000.290125	11.037683	-0.052350	4.815691
254.325930	8000.346093	11.042688	-0.052367	4.815707
254.332266	8000.341919	11.047693	-0.052368	4.815706
254.238721	8000.289141	11.052698	-0.052351	4.815691
254.293417	8000.315649	11.057703	-0.052361	4.815699
254.301560	8000.318978	11.062707	-0.052362	4.815700
254.256872	8000.319313	11.067712	-0.052354	4.815700
254.415318	8000.306934	11.072717	-0.052384	4.815695
254.407867	8000.267301	11.077722	-0.052382	4.815684
254.381555	8000.309575	11.082727	-0.052377	4.815696
254.399028	8000.282092	11.087731	-0.052380	4.815688
254.371185	8000.290175	11.092736	-0.052375	4.815691
254.502570	8000.322200	11.097741	-0.052399	4.815700
254.290465	8000.317678	11.102746	-0.052360	4.815699
254.530271	8000.331179	11.107751	-0.052404	4.815702
254.544818	8000.301513	11.112755	-0.052407	4.815693
254.391892	8000.297953	11.117760	-0.052378	4.815693
254.482380	8000.337855	11.122765	-0.052395	4.815704
254.535350	8000.303475	11.127770	-0.052405	4.815694
254.768772	8000.337160	11.132775	-0.052448	4.815703
254.449103	8000.323414	11.137779	-0.052389	4.815700
254.574777	8000.317977	11.142784	-0.052412	4.815698
254.636920	8000.305100	11.147789	-0.052424	4.815694
254.553108	8000.270632	11.152794	-0.052408	4.815684
254.686597	8000.308030	11.157799	-0.052433	4.815695
254.685220	8000.306934	11.162803	-0.052432	4.815694
254.567802	8000.323169	11.167808	-0.052410	4.815700
254.526598	8000.323561	11.172813	-0.052403	4.815700
254.418533	8000.332475	11.177818	-0.052383	4.815703
254.655180	8000.350196	11.182823	-0.052427	4.815707
254.559513	8000.319805	11.187827	-0.052409	4.815699
254.721065	8000.318154	11.192832	-0.052439	4.815697
254.849325	8000.344791	11.197837	-0.052462	4.815705
254.595654	8000.337457	11.202842	-0.052415	4.815704
254.662176	8000.368428	11.207847	-0.052427	4.815712
254.758344	8000.342224	11.212851	-0.052445	4.815704
254.473970	8000.349339	11.217856	-0.052392	4.815708
254.488895	8000.346372	11.222861	-0.052395	4.815707
254.582197	8000.315851	11.227866	-0.052412	4.815697
254.574256	8000.311445	11.232871	-0.052411	4.815696
254.688204	8000.295139	11.237875	-0.052432	4.815691
254.673677	8000.323725	11.242880	-0.052429	4.815699
254.651103	8000.323352	11.247885	-0.052425	4.815699
254.555563	8000.301505	11.252890	-0.052407	4.815693
254.452700	8000.351077	11.257895	-0.052388	4.815708
254.587250	8000.331904	11.262899	-0.052413	4.815702
254.561211	8000.318661	11.267904	-0.052408	4.815698
254.595181	8000.316004	11.272909	-0.052414	4.815697
254.494087	8000.323963	11.277914	-0.052395	4.815700
254.501610	8000.302725	11.282919	-0.052396	4.815694
254.504439	8000.282477	11.287923	-0.052397	4.815688
254.729361	8000.319227	11.292928	-0.052439	4.815698
254.765828	8000.329423	11.297933	-0.052445	4.815700
254.678360	8000.299166	11.302938	-0.052429	4.815692
254.611252	8000.320490	11.307943	-0.052416	4.815699
254.757853	8000.316461	11.312947	-0.052444	4.815697
254.649417	8000.333910	11.317952	-0.052423	4.815702
254.661419	8000.327693	11.322957	-0.052426	4.815700
254.613509	8000.320501	11.327962	-0.052417	4.815699
254.697751	8000.341083	11.332967	-0.052432	4.815704
254.591332	8000.366039	11.337971	-0.052412	4.815712
254.621406	8000.361183	11.342976	-0.052418	4.815710
254.714274	8000.327452	11.347981	-0.052435	4.815700
254.506858	8000.308057	11.352986	-0.052396	4.815695
254.595344	8000.321234	11.357991	-0.052413	4.815699
254.667861	8000.323474	11.362995	-0.052426	4.815699
254.539815	8000.322454	11.368000	-0.052402	4.815700
254.611976	8000.336433	11.373005	-0.052416	4.815703
254.517716	8000.315675	11.378010	-0.052398	4.815698
254.712546	8000.364748	11.383015	-0.052434	4.815711
254.762354	8000.328181	11.388019	-0.052443	4.815700
254.549635	8000.326852	11.393024	-0.052404	4.815701
254.806024	8000.333149	11.398029	-0.052451	4.815701
254.600850	8000.302046	11.403034	-0.052413	4.815693
254.657077	8000.340324	11.408039	-0.052424	4.815704
254.819456	8000.341890	11.413043	-0.052454	4.815704
254.593340	8000.336072	11.418048	-0.052412	4.815703
254.549157	8000.326805	11.423053	-0.052403	4.815701
254.344096	8000.278621	11.428058	-0.052365	4.815688
254.586701	8000.330605	11.433063	-0.052410	4.815702
254.546777	8000.309663	11.438067	-0.052403	4.815696
254.500802	8000.311045	11.443072	-0.052394	4.815696
254.954446	8000.322685	11.448077	-0.052478	4.815698
254.777164	8000.309118	11.453082	-0.052445	4.815695
254.695704	8000.336616	11.458087	-0.052430	4.815703
254.749138	8000.326801	11.463091	-0.052440	4.815700
254.745616	8000.302180	11.468096	-0.052439	4.815693
254.671689	8000.318055	11.473101	-0.052425	4.815698
254.459536	8000.304990	11.478106	-0.052386	4.815695
254.840389	8000.334665	11.483111	-0.052457	4.815702
254.868270	8000.305215	11.488115	-0.052462	4.815693
254.649332	8000.351832	11.493120	-0.052421	4.815708
254.909759	8000.357128	11.498125	-0.052469	4.815708
254.716340	8000.328351	11.503130	-0.052433	4.815700
254.600667	8000.332870	11.508135	-0.052412	4.815702
254.588773	8000.342280	11.513139	-0.052409	4.815705
254.641388	8000.327113	11.518144	-0.052419	4.815700
254.674381	8000.348997	11.523149	-0.052425	4.815707
254.644992	8000.312210	11.528154	-0.052419	4.815696
254.694886	8000.340776	11.533159	-0.052429	4.815704
254.772051	8000.302518	11.538163	-0.052443	4.815693
254.758058	8000.320435	11.543168	-0.052440	4.815698
254.738141	8000.354272	11.548173	-0.052437	4.815708
254.792182	8000.320977	11.553178	-0.052447	4.815698
254.788608	8000.348673	11.558183	-0.052446	4.815706
254.802002	8000.326462	11.563187	-0.052448	4.815700
254.809775	8000.315905	11.568192	-0.052450	4.815696
254.767374	8000.321616	11.573197	-0.052442	4.815698
254.832683	8000.302384	11.578202	-0.052454	4.815692
254.731784	8000.337040	11.583207	-0.052435	4.815703
254.701033	8000.315179	11.588211	-0.052429	4.815697
254.663699	8000.317768	11.593216	-0.052422	4.815698
254.681299	8000.343673	11.598221	-0.052425	4.815705
254.634403	8000.308737	11.603226	-0.052416	4.815695
254.569376	8000.341841	11.608231	-0.052404	4.815705
254.685660	8000.309558	11.613235	-0.052426	4.815695
254.775781	8000.312084	11.618240	-0.052442	4.815695
254.763420	8000.327892	11.623245	-0.052440	4.815700
254.768191	8000.299135	11.628250	-0.052441	4.815692
254.926462	8000.351885	11.633255	-0.052470	4.815706
255.090102	8000.322507	11.638259	-0.052501	4.815697
254.616632	8000.328683	11.643264	-0.052413	4.815701
254.725237	8000.327239	11.648269	-0.052433	4.815700
254.701637	8000.312969	11.653274	-0.052428	4.815696
254.799662	8000.340181	11.658279	-0.052446	4.815704
254.776179	8000.307761	11.663283	-0.052442	4.815694
254.600376	8000.335860	11.668288	-0.052409	4.815703
254.774259	8000.329071	11.673293	-0.052441	4.815700
254.589882	8000.291900	11.678298	-0.052407	4.815690
254.676740	8000.313592	11.683303	-0.052423	4.815696
254.947387	8000.317986	11.688307	-0.052473	4.815696
254.716470	8000.329173	11.693312	-0.052430	4.815701
254.835680	8000.336444	11.698317	-0.052452	4.815702
254.774612	8000.316225	11.703322	-0.052441	4.815697
254.729860	8000.349658	11.708327	-0.052433	4.815707
254.650117	8000.305646	11.713331	-0.052418	4.815694
254.841523	8000.292736	11.718336	-0.052453	4.815690
255.079577	8000.327564	11.723341	-0.052498	4.815699
254.665147	8000.277043	11.728346	-0.052420	4.815686
254.938437	8000.342340	11.733351	-0.052471	4.815704
254.982724	8000.333444	11.738355	-0.052479	4.815701
254.727376	8000.318608	11.743360	-0.052432	4.815698
254.691742	8000.352190	11.748365	-0.052425	4.815708
254.766530	8000.281862	11.753370	-0.052439	4.815687
254.742833	8000.317772	11.758375	-0.052434	4.815697
254.743750	8000.319916	11.763379	-0.052434	4.815698
254.737470	8000.327282	11.768384	-0.052433	4.815700
254.791713	8000.333496	11.773389	-0.052443	4.815702
254.552113	8000.302901	11.778394	-0.052398	4.815694
254.871456	8000.324102	11.783399	-0.052458	4.815699
255.061866	8000.303701	11.788403	-0.052493	4.815692
254.690987	8000.317952	11.793408	-0.052424	4.815698
254.681077	8000.329529	11.798413	-0.052422	4.815701
254.841626	8000.277679	11.803418	-0.052452	4.815685
254.727767	8000.309988	11.808423	-0.052431	4.815695
254.795827	8000.305750	11.813427	-0.052443	4.815694
254.737887	8000.334697	11.818432	-0.052432	4.815702
254.970987	8000.348090	11.823437	-0.052476	4.815705
254.806707	8000.317652	11.828442	-0.052445	4.815697
254.818013	8000.360538	11.833447	-0.052447	4.815710
254.890342	8000.296576	11.838451	-0.052461	4.815690
255.008950	8000.311311	11.843456	-0.052483	4.815694
254.950142	8000.326364	11.848461	-0.052472	4.815699
255.035260	8000.313861	11.853466	-0.052487	4.815695
254.900788	8000.344768	11.858471	-0.052462	4.815705
254.987350	8000.331221	11.863475	-0.052478	4.815700
254.772364	8000.334125	11.868480	-0.052438	4.815702
254.880864	8000.355102	11.873485	-0.052458	4.815708
254.718193	8000.343909	11.878490	-0.052428	4.815705
254.853616	8000.367458	11.883495	-0.052453	4.815711
254.879992	8000.363610	11.888499	-0.052458	4.815710
254.763241	8000.361705	11.893504	-0.052436	4.815710
254.729073	8000.357940	11.898509	-0.052430	4.815709
254.737815	8000.339924	11.903514	-0.052431	4.815704
254.858725	8000.370712	11.908519	-0.052454	4.815712
254.859956	8000.320542	11.913523	-0.052454	4.815698
254.834579	8000.335072	11.918528	-0.052449	4.815702
254.821993	8000.325251	11.923533	-0.052447	4.815699
254.739043	8000.306812	11.928538	-0.052431	4.815694
254.710635	8000.334105	11.933543	-0.052426	4.815702
254.846069	8000.309607	11.938547	-0.052451	4.815695
254.999612	8000.320639	11.943552	-0.052479	4.815697
254.919297	8000.357764	11.948557	-0.052464	4.815708
254.764451	8000.326412	11.953562	-0.052435	4.815700
254.787303	8000.341725	11.958567	-0.052440	4.815704
255.001948	8000.298228	11.963571	-0.052479	4.815690
254.789039	8000.321453	11.968576	-0.052440	4.815698
255.095883	8000.336045	11.973581	-0.052497	4.815701
254.894961	8000.310350	11.978586	-0.052459	4.815695
254.788415	8000.341710	11.983591	-0.052439	4.815704
254.864236	8000.320514	11.988595	-0.052453	4.815698
254.878416	8000.313264	11.993600	-0.052456	4.815695
254.837366	8000.344622	11.998605	-0.052448	4.815705
254.573526	8000.300820	12.003610	-0.052399	4.815693
254.651402	8000.306351	12.008615	-0.052414	4.815695
254.873174	8000.330237	12.013619	-0.052455	4.815700
254.899850	8000.345612	12.018624	-0.052460	4.815705
255.016662	8000.364589	12.023629	-0.052481	4.815710
255.023570	8000.316647	12.028634	-0.052483	4.815696
254.766733	8000.338090	12.033639	-0.052435	4.815703
254.851809	8000.329857	12.038643	-0.052450	4.815700
255.032904	8000.350946	12.043648	-0.052484	4.815706
254.912328	8000.348979	12.048653	-0.052462	4.815706
254.861079	8000.307566	12.053658	-0.052452	4.815694
254.812065	8000.353742	12.058663	-0.052443	4.815708
254.913421	8000.327623	12.063667	-0.052461	4.815700
254.688068	8000.335697	12.068672	-0.052419	4.815703
255.075516	8000.352668	12.073677	-0.052492	4.815706
255.048908	8000.314858	12.078682	-0.052486	4.815695
254.986571	8000.335192	12.083687	-0.052475	4.815701
255.036820	8000.329597	12.088691	-0.052484	4.815700
255.021308	8000.302645	12.093696	-0.052481	4.815692
254.936004	8000.350367	12.098701	-0.052465	4.815706
254.661727	8000.324546	12.103706	-0.052414	4.815700
254.896282	8000.363588	12.108711	-0.052458	4.815710
254.754063	8000.347389	12.113715	-0.052431	4.815706
254.709933	8000.315701	12.118720	-0.052423	4.815697
254.978511	8000.372380	12.123725	-0.052473	4.815712
254.995101	8000.327798	12.128730	-0.052476	4.815699
254.698078	8000.341114	12.133735	-0.052420	4.815705
254.882810	8000.340908	12.138739	-0.052455	4.815704
254.867283	8000.303278	12.143744	-0.052452	4.815693
254.941888	8000.330110	12.148749	-0.052466	4.815700
254.819291	8000.321704	12.153754	-0.052443	4.815698
254.999499	8000.341711	12.158759	-0.052476	4.815703
255.026317	8000.338938	12.163763	-0.052481	4.815702
254.900479	8000.320869	12.168768	-0.052458	4.815698
255.105148	8000.328461	12.173773	-0.052496	4.815699
255.013616	8000.329102	12.178778	-0.052478	4.815700
254.913327	8000.361632	12.183783	-0.052460	4.815710
254.884327	8000.340867	12.188787	-0.052454	4.815704
254.909327	8000.333793	12.193792	-0.052459	4.815701
254.937769	8000.353468	12.198797	-0.052464	4.815707
254.651430	8000.308233	12.203802	-0.052411	4.815695
254.913350	8000.343449	12.208807	-0.052459	4.815704
255.063174	8000.331998	12.213811	-0.052487	4.815700
254.898329	8000.343191	12.218816	-0.052456	4.815704
254.952137	8000.361143	12.223821	-0.052466	4.815709
255.043025	8000.309228	12.228826	-0.052483	4.815694
255.218219	8000.354780	12.233831	-0.052516	4.815706
255.183848	8000.311505	12.238835	-0.052509	4.815694
254.998315	8000.305279	12.243840	-0.052475	4.815693
255.213141	8000.337594	12.248845	-0.052515	4.815701
255.023528	8000.314217	12.253850	-0.052479	4.815695
255.063565	8000.352232	12.258855	-0.052487	4.815706
254.959118	8000.352663	12.263859	-0.052467	4.815707
254.825057	8000.318445	12.268864	-0.052442	4.815697
254.918461	8000.341312	12.273869	-0.052459	4.815704
254.866688	8000.322312	12.278874	-0.052450	4.815698
255.044887	8000.355099	12.283879	-0.052483	4.815707
255.121584	8000.345663	12.288883	-0.052497	4.815704
255.092438	8000.329166	12.293888	-0.052491	4.815699
255.181717	8000.355169	12.298893	-0.052508	4.815706
255.208142	8000.322493	12.303898	-0.052513	4.815697
255.000746	8000.335130	12.308903	-0.052474	4.815701
255.264900	8000.338351	12.313907	-0.052523	4.815701
255.053634	8000.348790	12.318912	-0.052484	4.815705
254.985638	8000.361558	12.323917	-0.052471	4.815709
254.921827	8000.324211	12.328922	-0.052459	4.815699
255.035559	8000.324986	12.333927	-0.052480	4.815698
254.949509	8000.308632	12.338931	-0.052464	4.815694
254.982888	8000.302762	12.343936	-0.052470	4.815692
255.141956	8000.337374	12.348941	-0.052500	4.815701
254.870115	8000.311593	12.353946	-0.052449	4.815695
254.835131	8000.323830	12.358951	-0.052443	4.815699
254.937542	8000.325489	12.363955	-0.052462	4.815699
255.105322	8000.303652	12.368960	-0.052493	4.815692
255.155103	8000.326878	12.373965	-0.052502	4.815698
255.232040	8000.308903	12.378970	-0.052516	4.815693
255.191517	8000.339202	12.383975	-0.052509	4.815702
255.132747	8000.313682	12.388979	-0.052497	4.815695
255.089515	8000.309769	12.393984	-0.052489	4.815694
255.161717	8000.334427	12.398989	-0.052503	4.815700
254.967030	8000.301358	12.403994	-0.052466	4.815692
255.039460	8000.335629	12.408999	-0.052480	4.815701
255.066410	8000.317909	12.414003	-0.052485	4.815696
255.040059	8000.318542	12.419008	-0.052480	4.815696
255.102023	8000.356914	12.424013	-0.052491	4.815707
255.028559	8000.322613	12.429018	-0.052477	4.815698
254.953337	8000.341670	12.434023	-0.052463	4.815704
254.833019	8000.310879	12.439027	-0.052441	4.815695
254.705302	8000.290645	12.444032	-0.052417	4.815690
254.850182	8000.321822	12.449037	-0.052444	4.815698
254.973640	8000.298197	12.454042	-0.052467	4.815691
254.867064	8000.345574	12.459047	-0.052447	4.815705
255.116503	8000.331471	12.464051	-0.052493	4.815700
255.103895	8000.320583	12.469056	-0.052491	4.815697
255.120759	8000.362492	12.474061	-0.052494	4.815709
254.933129	8000.303913	12.479066	-0.052459	4.815693
255.143138	8000.335082	12.484071	-0.052498	4.815701
254.947557	8000.340437	12.489075	-0.052462	4.815703
254.999853	8000.311384	12.494080	-0.052471	4.815695
255.090367	8000.343814	12.499085	-0.052488	4.815704
254.988106	8000.318654	12.504090	-0.052469	4.815697
254.951075	8000.331926	12.509095	-0.052462	4.815701
254.987223	8000.313288	12.514099	-0.052469	4.815695
254.940716	8000.301848	12.519104	-0.052460	4.815692
254.970368	8000.372794	12.524109	-0.052465	4.815713
255.007653	8000.321075	12.529114	-0.052472	4.815697
255.212202	8000.362833	12.534119	-0.052510	4.815709
255.147477	8000.316929	12.539123	-0.052498	4.815695
254.976947	8000.313082	12.544128	-0.052466	4.815695
255.136734	8000.351977	12.549133	-0.052496	4.815706
255.061683	8000.336869	12.554138	-0.052482	4.815702
255.004960	8000.355160	12.559143	-0.052471	4.815707
254.971383	8000.339659	12.564147	-0.052465	4.815703
254.986095	8000.337756	12.569152	-0.052468	4.815702
255.078562	8000.358472	12.574157	-0.052485	4.815708
254.953708	8000.313726	12.579162	-0.052461	4.815695
255.104340	8000.340727	12.584167	-0.052489	4.815703
254.916056	8000.334456	12.589171	-0.052454	4.815702
254.946785	8000.314662	12.594176	-0.052460	4.815696
255.077403	8000.311441	12.599181	-0.052484	4.815694
255.154246	8000.312684	12.604186	-0.052498	4.815694
255.105018	8000.359925	12.609191	-0.052489	4.815708
255.141604	8000.328481	12.614195	-0.052496	4.815699
255.283722	8000.340395	12.619200	-0.052522	4.815702
255.280684	8000.364897	12.624205	-0.052522	4.815709
255.205282	8000.330565	12.629210	-0.052507	4.815699
255.256167	8000.337792	12.634215	-0.052517	4.815701
255.099439	8000.297866	12.639219	-0.052488	4.815690
254.826285	8000.317976	12.644224	-0.052437	4.815697
255.221943	8000.324403	12.649229	-0.052510	4.815697
255.114114	8000.318372	12.654234	-0.052490	4.815696
255.182922	8000.347246	12.659239	-0.052503	4.815704
255.115821	8000.344013	12.664243	-0.052490	4.815704
255.073685	8000.311289	12.669248	-0.052482	4.815694
255.055475	8000.329138	12.674253	-0.052479	4.815700
254.866206	8000.319648	12.679258	-0.052444	4.815698
255.073914	8000.327289	12.684263	-0.052482	4.815699
255.170277	8000.320308	12.689267	-0.052500	4.815696
254.999410	8000.322862	12.694272	-0.052468	4.815698
255.221807	8000.355300	12.699277	-0.052509	4.815706
255.184903	8000.302375	12.704282	-0.052502	4.815691
255.064281	8000.320694	12.709287	-0.052480	4.815697
255.138389	8000.317621	12.714291	-0.052494	4.815696
255.165727	8000.308450	12.719296	-0.052499	4.815693
255.243951	8000.356695	12.724301	-0.052513	4.815707
255.392019	8000.307845	12.729306	-0.052541	4.815692
255.376781	8000.344962	12.734311	-0.052538	4.815703
255.354828	8000.316837	12.739315	-0.052534	4.815695
255.337605	8000.299467	12.744320	-0.052530	4.815690
255.343268	8000.360413	12.749325	-0.052531	4.815707
255.507279	8000.315026	12.754330	-0.052562	4.815693
255.444698	8000.330018	12.759335	-0.052550	4.815698
255.380831	8000.338582	12.764339	-0.052538	4.815701
255.380797	8000.305475	12.769344	-0.052538	4.815691
255.491026	8000.348903	12.774349	-0.052558	4.815703
255.416306	8000.389323	12.779354	-0.052545	4.815715
255.438191	8000.358708	12.784359	-0.052548	4.815706
255.597143	8000.359151	12.789363	-0.052578	4.815706
255.368448	8000.334071	12.794368	-0.052535	4.815700
255.446867	8000.356694	12.799373	-0.052550	4.815706
255.347146	8000.309153	12.804378	-0.052531	4.815692
255.333876	8000.322812	12.809383	-0.052529	4.815696
255.337720	8000.319664	12.814387	-0.052529	4.815695
255.316848	8000.311844	12.819392	-0.052525	4.815693
255.219228	8000.367908	12.824397	-0.052507	4.815710
255.141027	8000.324988	12.829402	-0.052492	4.815698
255.261233	8000.354698	12.834407	-0.052515	4.815706
255.205688	8000.335636	12.839411	-0.052504	4.815701
255.197814	8000.326960	12.844416	-0.052503	4.815698
255.131716	8000.351504	12.849421	-0.052490	4.815706
255.289504	8000.302812	12.854426	-0.052520	4.815691
255.224805	8000.339124	12.859431	-0.052508	4.815702
255.130291	8000.338649	12.864435	-0.052490	4.815702
255.069510	8000.310961	12.869440	-0.052479	4.815694
255.354641	8000.339081	12.874445	-0.052532	4.815701
255.357552	8000.295344	12.879450	-0.052532	4.815688
255.207497	8000.324930	12.884455	-0.052504	4.815698
255.547383	8000.315502	12.889459	-0.052567	4.815693
255.337467	8000.314217	12.894464	-0.052528	4.815694
255.390932	8000.340706	12.899469	-0.052538	4.815701
255.408836	8000.347397	12.904474	-0.052541	4.815703
255.241543	8000.331857	12.909479	-0.052510	4.815700
255.297612	8000.340237	12.914483	-0.052520	4.815702
255.142957	8000.314225	12.919488	-0.052491	4.815695
255.265633	8000.326891	12.924493	-0.052514	4.815698
255.188060	8000.298930	12.929498	-0.052500	4.815690
255.056096	8000.309590	12.934503	-0.052475	4.815694
255.114107	8000.324407	12.939507	-0.052486	4.815698
254.966776	8000.309193	12.944512	-0.052458	4.815694
255.069969	8000.311932	12.949517	-0.052477	4.815695
255.139051	8000.307710	12.954522	-0.052490	4.815693
255.201324	8000.302309	12.959527	-0.052502	4.815691
255.124968	8000.308535	12.964531	-0.052487	4.815693
255.178144	8000.275226	12.969536	-0.052497	4.815683
255.435158	8000.334921	12.974541	-0.052545	4.815700
255.172029	8000.305010	12.979546	-0.052496	4.815692
255.292921	8000.341137	12.984551	-0.052518	4.815702
255.634576	8000.342416	12.989555	-0.052582	4.815701
255.392390	8000.332064	12.994560	-0.052537	4.815699
255.413060	8000.364426	12.999565	-0.052541	4.815708
255.306139	8000.300752	13.004570	-0.052521	4.815690
255.236127	8000.328436	13.009575	-0.052507	4.815699
255.355805	8000.359204	13.014579	-0.052530	4.815707
255.127934	8000.330934	13.019584	-0.052487	4.815700
255.232138	8000.359316	13.024589	-0.052507	4.815708
255.213819	8000.325911	13.029594	-0.052503	4.815698
255.279985	8000.353674	13.034599	-0.052515	4.815706
255.350211	8000.351607	13.039603	-0.052528	4.815705
255.366828	8000.344396	13.044608	-0.052531	4.815703
255.120218	8000.370276	13.049613	-0.052485	4.815711
255.324247	8000.313794	13.054618	-0.052523	4.815694
255.327297	8000.312769	13.059623	-0.052524	4.815694
255.377782	8000.314651	13.064627	-0.052533	4.815694
255.253235	8000.301942	13.069632	-0.052510	4.815691
255.426886	8000.338927	13.074637	-0.052542	4.815701
255.219890	8000.319539	13.079642	-0.052503	4.815696
255.120964	8000.322194	13.084647	-0.052485	4.815697
255.254863	8000.331839	13.089651	-0.052510	4.815700
255.272782	8000.289415	13.094656	-0.052513	4.815687
255.294200	8000.324992	13.099661	-0.052517	4.815697
255.337874	8000.304341	13.104666	-0.052525	4.815691
255.206681	8000.319285	13.109671	-0.052501	4.815696
255.306742	8000.363615	13.114675	-0.052519	4.815709
255.285735	8000.312015	13.119680	-0.052515	4.815694
255.452220	8000.315784	13.124685	-0.052546	4.815694
255.411380	8000.339671	13.129690	-0.052538	4.815701
255.231546	8000.314318	13.134695	-0.052505	4.815695
255.665950	8000.336324	13.139699	-0.052586	4.815699
255.630135	8000.323990	13.144704	-0.052579	4.815695
255.534217	8000.350185	13.149709	-0.052561	4.815704
255.240064	8000.299482	13.154714	-0.052506	4.815690
255.436687	8000.352856	13.159719	-0.052543	4.815705
255.360390	8000.356948	13.164723	-0.052528	4.815706
255.218673	8000.309792	13.169728	-0.052502	4.815693
255.324494	8000.370232	13.174733	-0.052522	4.815710
255.375562	8000.295246	13.179738	-0.052531	4.815688
255.301695	8000.308987	13.184743	-0.052517	4.815693
255.325033	8000.334986	13.189747	-0.052521	4.815700
255.502427	8000.320780	13.194752	-0.052554	4.815695
255.506719	8000.338995	13.199757	-0.052555	4.815700
255.491750	8000.336609	13.204762	-0.052552	4.815700
255.476032	8000.331009	13.209767	-0.052549	4.815698
255.339734	8000.337328	13.214771	-0.052524	4.815701
255.197694	8000.307250	13.219776	-0.052497	4.815693
255.480913	8000.342814	13.224781	-0.052550	4.815702
255.357350	8000.340798	13.229786	-0.052527	4.815702
255.305121	8000.332468	13.234791	-0.052517	4.815700
255.445195	8000.329400	13.239795	-0.052543	4.815698
255.338387	8000.293489	13.244800	-0.052523	4.815688
255.375273	8000.348537	13.249805	-0.052530	4.815704
255.296248	8000.316281	13.254810	-0.052515	4.815695
255.522780	8000.342381	13.259815	-0.052557	4.815701
255.469140	8000.325486	13.264819	-0.052547	4.815697
255.385692	8000.314513	13.269824	-0.052531	4.815694
255.527436	8000.350979	13.274829	-0.052558	4.815704
255.456218	8000.318850	13.279834	-0.052544	4.815695
255.328104	8000.329573	13.284839	-0.052521	4.815699
255.481555	8000.352349	13.289843	-0.052549	4.815705
255.571223	8000.334581	13.294848	-0.052566	4.815699
255.531898	8000.344613	13.299853	-0.052558	4.815702
255.387957	8000.311301	13.304858	-0.052531	4.815693
255.493168	8000.336496	13.309863	-0.052551	4.815700
255.441504	8000.338852	13.314867	-0.052541	4.815701
255.401689	8000.331792	13.319872	-0.052534	4.815699
255.311100	8000.339922	13.324877	-0.052517	4.815702
255.525177	8000.324177	13.329882	-0.052557	4.815696
255.540551	8000.320150	13.334887	-0.052559	4.815695
255.293047	8000.332135	13.339891	-0.052513	4.815700
255.418743	8000.312817	13.344896	-0.052536	4.815693
255.398370	8000.334902	13.349901	-0.052533	4.815700
255.200378	8000.310321	13.354906	-0.052496	4.815694
255.406170	8000.341422	13.359911	-0.052534	4.815702
255.430664	8000.358898	13.364915	-0.052538	4.815707
255.256649	8000.317623	13.369920	-0.052506	4.815695
255.294047	8000.338512	13.374925	-0.052513	4.815701
255.393547	8000.311294	13.379930	-0.052531	4.815693
255.442138	8000.322755	13.384935	-0.052540	4.815696
255.300137	8000.319372	13.389939	-0.052514	4.815696
255.332464	8000.329501	13.394944	-0.052520	4.815699
255.485813	8000.343733	13.399949	-0.052548	4.815702
255.442341	8000.318462	13.404954	-0.052540	4.815695
255.284131	8000.342576	13.409959	-0.052510	4.815703
255.641378	8000.328092	13.414963	-0.052577	4.815697
255.433992	8000.307629	13.419968	-0.052538	4.815692
255.344021	8000.311498	13.424973	-0.052521	4.815693
255.233860	8000.320378	13.429978	-0.052501	4.815696
255.272257	8000.317792	13.434983	-0.052508	4.815695
255.292549	8000.360825	13.439987	-0.052512	4.815708
255.264129	8000.301631	13.444992	-0.052506	4.815691
255.402018	8000.316679	13.449997	-0.052532	4.815695
255.229018	8000.292505	13.455002	-0.052500	4.815688
255.333166	8000.336902	13.460007	-0.052519	4.815701
255.545487	8000.336077	13.465011	-0.052558	4.815700
255.492996	8000.312794	13.470016	-0.052548	4.815693
255.437796	8000.337516	13.475021	-0.052538	4.815700
255.594992	8000.330456	13.480026	-0.052567	4.815698
255.575618	8000.321592	13.485031	-0.052564	4.815695
255.574844	8000.335454	13.490035	-0.052563	4.815699
255.400178	8000.308049	13.495040	-0.052531	4.815692
255.604083	8000.346594	13.500045	-0.052569	4.815702
255.356486	8000.325477	13.505050	-0.052523	4.815697
255.342433	8000.338055	13.510055	-0.052520	4.815701
255.559695	8000.347988	13.515059	-0.052560	4.815703
255.456506	8000.296120	13.520064	-0.052541	4.815688
255.499098	8000.329906	13.525069	-0.052549	4.815698
255.477707	8000.328483	13.530074	-0.052545	4.815698
255.336824	8000.349676	13.535079	-0.052518	4.815705
255.327902	8000.333509	13.540083	-0.052517	4.815700
255.477677	8000.328463	13.545088	-0.052544	4.815698
255.402362	8000.344316	13.550093	-0.052530	4.815703
255.429266	8000.324460	13.555098	-0.052535	4.815697
255.335792	8000.333611	13.560103	-0.052518	4.815700
255.645764	8000.352526	13.565107	-0.052575	4.815704
255.605343	8000.316626	13.570112	-0.052568	4.815694
255.451785	8000.336545	13.575117	-0.052539	4.815700
255.451856	8000.340811	13.580122	-0.052539	4.815701
255.419095	8000.324255	13.585127	-0.052533	4.815697
255.409571	8000.345449	13.590131	-0.052531	4.815703
255.217499	8000.283594	13.595136	-0.052495	4.815686
255.405133	8000.352838	13.600141	-0.052530	4.815705
255.354794	8000.335997	13.605146	-0.052521	4.815700
255.337803	8000.334646	13.610151	-0.052517	4.815700
255.623798	8000.332884	13.615155	-0.052571	4.815698
255.354214	8000.313545	13.620160	-0.052520	4.815694
255.359454	8000.360604	13.625165	-0.052521	4.815708
255.393326	8000.333387	13.630170	-0.052528	4.815700
255.416009	8000.336953	13.635175	-0.052532	4.815700
255.481999	8000.355103	13.640179	-0.052544	4.815705
255.370730	8000.306307	13.645184	-0.052523	4.815692
255.497964	8000.348944	13.650189	-0.052547	4.815704
255.324627	8000.323696	13.655194	-0.052514	4.815697
255.249050	8000.324596	13.660199	-0.052500	4.815698
255.393892	8000.344028	13.665203	-0.052527	4.815703
255.335668	8000.319585	13.670208	-0.052516	4.815696
255.286485	8000.331591	13.675213	-0.052507	4.815700
255.230858	8000.321071	13.680218	-0.052497	4.815697
255.283499	8000.298430	13.685223	-0.052506	4.815690
255.356435	8000.323100	13.690227	-0.052520	4.815697
255.243542	8000.311648	13.695232	-0.052499	4.815694
255.334790	8000.359038	13.700237	-0.052516	4.815707
255.333835	8000.341932	13.705242	-0.052515	4.815702
255.536865	8000.338821	13.710247	-0.052553	4.815700
255.540244	8000.341005	13.715251	-0.052554	4.815701
255.351537	8000.313371	13.720256	-0.052518	4.815694
255.349431	8000.363514	13.725261	-0.052518	4.815709
255.397842	8000.344008	13.730266	-0.052527	4.815703
255.325229	8000.343888	13.735271	-0.052513	4.815703
255.417015	8000.334697	13.740275	-0.052530	4.815700
255.176472	8000.289138	13.745280	-0.052485	4.815688
255.557700	8000.316685	13.750285	-0.052556	4.815694
255.532566	8000.329082	13.755290	-0.052552	4.815698
255.442946	8000.284909	13.760295	-0.052535	4.815685
255.677816	8000.323957	13.765299	-0.052578	4.815695
255.604357	8000.303537	13.770304	-0.052565	4.815690
255.666440	8000.330166	13.775309	-0.052576	4.815697
255.358167	8000.331553	13.780314	-0.052519	4.815699
255.489529	8000.325140	13.785319	-0.052543	4.815697
255.615798	8000.344271	13.790323	-0.052567	4.815702
255.368466	8000.329565	13.795328	-0.052520	4.815699
255.528406	8000.324685	13.800333	-0.052550	4.815696
255.377209	8000.313678	13.805338	-0.052522	4.815694
255.453603	8000.323456	13.810343	-0.052536	4.815696
255.503033	8000.319982	13.815347	-0.052545	4.815695
255.598644	8000.310853	13.820352	-0.052563	4.815692
255.525615	8000.332081	13.825357	-0.052549	4.815699
255.296336	8000.361446	13.830362	-0.052506	4.815708
255.569132	8000.321031	13.835367	-0.052557	4.815695
255.541767	8000.349408	13.840371	-0.052552	4.815704
255.414645	8000.301422	13.845376	-0.052528	4.815690
255.571999	8000.339210	13.850381	-0.052558	4.815700
255.608772	8000.336598	13.855386	-0.052564	4.815700
255.507881	8000.346696	13.860391	-0.052545	4.815703
255.501118	8000.379679	13.865395	-0.052544	4.815713
255.583530	8000.346845	13.870400	-0.052559	4.815703
255.539564	8000.365343	13.875405	-0.052551	4.815708
255.389595	8000.347949	13.880410	-0.052523	4.815704
255.367459	8000.357192	13.885415	-0.052519	4.815707
255.624248	8000.346414	13.890419	-0.052567	4.815702
255.405512	8000.305479	13.895424	-0.052526	4.815691
255.523686	8000.339427	13.900429	-0.052548	4.815701
255.640584	8000.318899	13.905434	-0.052569	4.815694
255.595409	8000.308548	13.910439	-0.052561	4.815691
255.491693	8000.369851	13.915443	-0.052542	4.815710
255.562454	8000.327218	13.920448	-0.052555	4.815697
255.618770	8000.369769	13.925453	-0.052565	4.815709
255.514031	8000.333892	13.930458	-0.052546	4.815699
255.442989	8000.348746	13.935463	-0.052532	4.815704
255.447709	8000.327461	13.940467	-0.052533	4.815698
255.314408	8000.323152	13.945472	-0.052508	4.815697
255.531213	8000.336281	13.950477	-0.052548	4.815700
255.823495	8000.312199	13.955482	-0.052603	4.815691
255.548234	8000.328002	13.960487	-0.052551	4.815697
255.622424	8000.353761	13.965491	-0.052565	4.815705
255.447593	8000.321014	13.970496	-0.052533	4.815696
255.528284	8000.345810	13.975501	-0.052548	4.815703
255.474846	8000.323580	13.980506	-0.052537	4.815696
255.686573	8000.335558	13.985511	-0.052577	4.815699
255.821734	8000.359105	13.990515	-0.052602	4.815705
255.583567	8000.368038	13.995520	-0.052558	4.815709
255.582276	8000.387230	14.000525	-0.052557	4.815715
255.615835	8000.360008	14.005530	-0.052563	4.815706
255.377410	8000.352921	14.010535	-0.052519	4.815705
255.506377	8000.409466	14.015539	-0.052543	4.815721
255.503780	8000.337879	14.020544	-0.052542	4.815700
255.538030	8000.344836	14.025549	-0.052549	4.815702
255.602422	8000.310641	14.030554	-0.052560	4.815692
255.485925	8000.333298	14.035559	-0.052539	4.815699
255.670598	8000.335227	14.040563	-0.052573	4.815699
255.523671	8000.316815	14.045568	-0.052546	4.815694
255.599680	8000.354348	14.050573	-0.052560	4.815705
255.653919	8000.339207	14.055578	-0.052570	4.815700
255.465268	8000.317981	14.060583	-0.052534	4.815695
255.589288	8000.358430	14.065587	-0.052558	4.815706
255.365241	8000.315274	14.070592	-0.052516	4.815695
255.698645	8000.331366	14.075597	-0.052578	4.815698
255.707181	8000.327228	14.080602	-0.052579	4.815696
255.522509	8000.322083	14.085607	-0.052545	4.815696
255.778063	8000.357197	14.090611	-0.052592	4.815705
255.651461	8000.340183	14.095616	-0.052569	4.815700
255.658183	8000.368047	14.100621	-0.052570	4.815709
255.662850	8000.354236	14.105626	-0.052571	4.815705
255.657116	8000.340255	14.110631	-0.052569	4.815700
255.637765	8000.369831	14.115635	-0.052566	4.815709
255.630418	8000.352621	14.120640	-0.052564	4.815704
255.454668	8000.358298	14.125645	-0.052532	4.815707
255.659422	8000.341334	14.130650	-0.052570	4.815701
255.581277	8000.319770	14.135655	-0.052555	4.815695
255.737620	8000.354338	14.140659	-0.052584	4.815704
255.804834	8000.382119	14.145664	-0.052596	4.815712
255.772163	8000.392258	14.150669	-0.052590	4.815715
255.598134	8000.385150	14.155674	-0.052558	4.815714
255.713254	8000.333629	14.160679	-0.052579	4.815698
255.599043	8000.369136	14.165683	-0.052558	4.815709
255.525883	8000.360465	14.170688	-0.052544	4.815707
255.777934	8000.348542	14.175693	-0.052591	4.815702
255.757385	8000.346066	14.180698	-0.052587	4.815702
255.689071	8000.344948	14.185703	-0.052574	4.815702
255.916228	8000.379601	14.190707	-0.052617	4.815711
255.849265	8000.321915	14.195712	-0.052604	4.815694
255.647344	8000.357063	14.200717	-0.052566	4.815705
255.800502	8000.343531	14.205722	-0.052595	4.815701
255.835041	8000.320596	14.210727	-0.052601	4.815694
255.583312	8000.349595	14.215731	-0.052554	4.815704
255.473412	8000.306160	14.220736	-0.052534	4.815691
255.694155	8000.339640	14.225741	-0.052575	4.815700
255.775081	8000.342017	14.230746	-0.052590	4.815700
255.594974	8000.342285	14.235751	-0.052556	4.815701
255.869311	8000.370231	14.240755	-0.052607	4.815708
255.768262	8000.328006	14.245760	-0.052588	4.815696
255.606201	8000.367006	14.250765	-0.052558	4.815709
255.502204	8000.358902	14.255770	-0.052538	4.815707
255.528906	8000.329433	14.260775	-0.052543	4.815698
255.416787	8000.343619	14.265779	-0.052522	4.815703
255.590611	8000.309068	14.270784	-0.052555	4.815692
255.645082	8000.347319	14.275789	-0.052565	4.815703
255.444316	7999.386315	14.280794	-0.052527	4.815423

255.511421	7996.106755	14.285799	-0.052537	4.814463
255.820766	7990.646136	14.290803	-0.052591	4.812864
255.555234	7983.952463	14.295808	-0.052537	4.810907
255.518803	7976.645730	14.300813	-0.052525	4.808768
255.519700	7969.048712	14.305818	-0.052521	4.806543
255.304520	7961.187740	14.310823	-0.052475	4.804241
255.500079	7953.363454	14.315827	-0.052507	4.801946
255.278714	7945.368480	14.320832	-0.052460	4.799602
255.413996	7937.467853	14.325837	-0.052480	4.797283
255.617469	7929.441231	14.330842	-0.052513	4.794925
255.183437	7921.367897	14.335847	-0.052426	4.792556
255.291110	7913.383931	14.340851	-0.052441	4.790209
255.258522	7905.413564	14.345856	-0.052430	4.787866
255.205007	7897.419245	14.350861	-0.052415	4.785514
255.354359	7889.435881	14.355866	-0.052437	4.783164
255.299786	7881.399605	14.360871	-0.052422	4.780798
255.175695	7873.411976	14.365875	-0.052393	4.778445
254.970737	7865.407167	14.370880	-0.052350	4.776086
255.102489	7857.392717	14.375885	-0.052369	4.773722
255.225185	7849.397950	14.380890	-0.052387	4.771363
254.864415	7841.351402	14.385895	-0.052314	4.768989
255.034187	7833.387354	14.390899	-0.052341	4.766636
254.967554	7825.368355	14.395904	-0.052323	4.764267
254.898528	7817.381858	14.400909	-0.052305	4.761906
254.793898	7809.403162	14.405914	-0.052280	4.759547
254.697074	7801.409576	14.410919	-0.052257	4.757181
254.837561	7793.414249	14.415923	-0.052277	4.754814
254.684022	7785.352173	14.420928	-0.052244	4.752426
254.847857	7777.302931	14.425933	-0.052269	4.750040
254.651038	7769.405405	14.430938	-0.052227	4.747699
254.554921	7761.277249	14.435943	-0.052204	4.745287
254.666525	7753.360456	14.440947	-0.052219	4.742937
254.608934	7745.302908	14.445952	-0.052203	4.740544
254.510232	7737.344645	14.450957	-0.052179	4.738180
254.476738	7729.371085	14.455962	-0.052168	4.735810
254.471476	7721.303161	14.460967	-0.052162	4.733410
254.545739	7713.306159	14.465971	-0.052170	4.731030
254.523203	7705.308086	14.470976	-0.052161	4.728649
254.508822	7697.293175	14.475981	-0.052153	4.726262
254.496304	7689.329473	14.480986	-0.052145	4.723889
254.314818	7681.318098	14.485991	-0.052106	4.721500
254.362035	7673.346244	14.490995	-0.052110	4.719122
254.238694	7665.361322	14.496000	-0.052081	4.716739
254.357826	7657.314487	14.501005	-0.052098	4.714336
254.352009	7649.285372	14.506010	-0.052092	4.711937
254.286221	7641.294358	14.511015	-0.052074	4.709548
254.529797	7633.336850	14.516019	-0.052114	4.707167
254.109980	7625.266908	14.521024	-0.052031	4.704754
254.046034	7617.318442	14.526029	-0.052014	4.702374
254.086484	7609.296594	14.531034	-0.052016	4.699971
253.968813	7601.286129	14.536039	-0.051989	4.697570
254.085038	7593.336481	14.541043	-0.052005	4.695186
254.112522	7585.298729	14.546048	-0.052005	4.692775
253.951811	7577.272292	14.551053	-0.051970	4.690366
253.932654	7569.319468	14.556058	-0.051961	4.687978
253.980757	7561.289030	14.561063	-0.051964	4.685565
254.067682	7553.289924	14.566067	-0.051975	4.683160
253.866804	7545.279900	14.571072	-0.051933	4.680751
254.093454	7537.322921	14.576077	-0.051970	4.678356
254.119264	7529.299507	14.581082	-0.051969	4.675940
253.715855	7521.204671	14.586087	-0.051889	4.673502
253.500715	7513.182378	14.591091	-0.051843	4.671085
253.649083	7505.165884	14.596096	-0.051866	4.668667
253.406458	7497.211897	14.601101	-0.051815	4.666267
253.505173	7489.249990	14.606106	-0.051828	4.663864
253.544427	7481.270238	14.611111	-0.051830	4.661454
253.730279	7473.203195	14.616115	-0.051860	4.659016
253.432088	7465.256393	14.621120	-0.051799	4.656613
253.410786	7457.235232	14.626125	-0.051790	4.654187
253.551586	7449.300213	14.631130	-0.051811	4.651785
253.490619	7441.166677	14.636135	-0.051794	4.649322
253.529460	7433.230376	14.641139	-0.051796	4.646917
253.508218	7425.244495	14.646144	-0.051787	4.644497
253.364526	7417.235775	14.651149	-0.051755	4.642068
253.408909	7409.220365	14.656154	-0.051757	4.639635
253.484508	7401.230793	14.661159	-0.051766	4.637210
253.403473	7393.217393	14.666163	-0.051746	4.634775
253.413624	7385.191938	14.671168	-0.051742	4.632336
253.146555	7377.163203	14.676173	-0.051687	4.629895
253.206481	7369.205817	14.681178	-0.051693	4.627474
253.203723	7361.163330	14.686183	-0.051688	4.625025
253.245077	7353.257332	14.691187	-0.051690	4.622617
253.183758	7345.194602	14.696192	-0.051673	4.620160
253.115188	7337.220132	14.701197	-0.051655	4.617729
253.017449	7329.181347	14.706202	-0.051632	4.615277
252.902446	7321.112117	14.711207	-0.051605	4.612814
253.124033	7313.142176	14.716211	-0.051641	4.610380
252.930756	7305.190899	14.721216	-0.051600	4.607950
252.693810	7297.156130	14.726221	-0.051550	4.605494
252.848940	7289.198846	14.731226	-0.051574	4.603060
252.883791	7281.144890	14.736231	-0.051575	4.600595
252.766243	7273.211651	14.741235	-0.051548	4.598166
252.698862	7265.204136	14.746240	-0.051530	4.595713
252.729226	7257.122360	14.751245	-0.051530	4.593235
252.788965	7249.105945	14.756250	-0.051536	4.590777
252.571532	7241.124909	14.761255	-0.051490	4.588327
252.672691	7233.115979	14.766259	-0.051504	4.585869
252.432569	7225.075589	14.771264	-0.051454	4.583398
252.445610	7217.137456	14.776269	-0.051451	4.580959
252.737951	7209.162153	14.781274	-0.051500	4.578506
252.625185	7201.142558	14.786279	-0.051474	4.576039
252.451757	7193.141734	14.791283	-0.051436	4.573575
252.458917	7185.095020	14.796288	-0.051432	4.571097
252.582887	7177.080605	14.801293	-0.051450	4.568627
252.424949	7169.152546	14.806298	-0.051416	4.566182
252.241619	7161.128752	14.811303	-0.051376	4.563706
252.493686	7153.185402	14.816307	-0.051418	4.561255
252.369739	7145.141791	14.821312	-0.051389	4.558770
252.201025	7137.178578	14.826317	-0.051353	4.556309
252.091729	7129.155861	14.831322	-0.051327	4.553828
252.013841	7121.088983	14.836327	-0.051307	4.551333
252.114476	7113.102272	14.841331	-0.051321	4.548861
252.095131	7105.083232	14.846336	-0.051312	4.546377
252.278778	7097.099686	14.851341	-0.051341	4.543904
251.990326	7089.147317	14.856346	-0.051282	4.541438
252.000298	7081.128180	14.861351	-0.051278	4.538950
252.065366	7073.168410	14.866355	-0.051285	4.536479
252.068493	7065.128931	14.871360	-0.051280	4.533983
251.889466	7057.081021	14.876365	-0.051242	4.531482
251.870321	7049.131924	14.881370	-0.051233	4.529010
251.816092	7041.102140	14.886375	-0.051218	4.526512
251.672827	7033.113555	14.891379	-0.051186	4.524026
251.640432	7025.095539	14.896384	-0.051174	4.521529
251.753752	7017.099908	14.901389	-0.051190	4.519038
251.898351	7009.157465	14.906394	-0.051212	4.516562
251.542882	7001.093210	14.911399	-0.051140	4.514046
251.736777	6993.041144	14.916403	-0.051171	4.511533
251.586754	6985.052324	14.921408	-0.051138	4.509038
251.377102	6977.071496	14.926413	-0.051094	4.506544
251.526552	6969.075083	14.931418	-0.051116	4.504044
251.624337	6961.079527	14.936423	-0.051129	4.501544
251.658796	6953.099928	14.941427	-0.051130	4.499046
251.475675	6945.113816	14.946432	-0.051091	4.496545
251.425507	6937.046297	14.951437	-0.051076	4.494017
251.598777	6929.040922	14.956442	-0.051103	4.491508
251.460341	6921.005221	14.961447	-0.051072	4.488987
251.619781	6913.066573	14.966451	-0.051096	4.486496
251.455268	6905.018316	14.971456	-0.051060	4.483968
251.234668	6897.051744	14.976461	-0.051014	4.481464
251.223827	6889.065648	14.981466	-0.051007	4.478953
251.216166	6881.069125	14.986471	-0.051000	4.476438
251.360188	6873.021887	14.991475	-0.051022	4.473906
250.988464	6865.013681	14.996480	-0.050947	4.471383
251.180822	6856.988859	15.001485	-0.050978	4.468855
251.196183	6849.046791	15.006490	-0.050975	4.466351
251.041412	6841.007296	15.011495	-0.050941	4.463814
250.988347	6833.041430	15.016499	-0.050926	4.461300
250.923260	6825.052558	15.021504	-0.050909	4.458777
250.900097	6817.039080	15.026509	-0.050899	4.456244
250.966905	6809.053723	15.031514	-0.050906	4.453720
250.982876	6800.974863	15.036519	-0.050904	4.451164
251.168351	6793.022692	15.041523	-0.050933	4.448648
250.822876	6785.000139	15.046528	-0.050863	4.446106
250.919469	6777.007940	15.051533	-0.050876	4.443573
250.970707	6769.032693	15.056538	-0.050880	4.441045
250.697531	6761.034947	15.061543	-0.050824	4.438506
250.896796	6753.050066	15.066547	-0.050856	4.435972
250.785023	6744.978748	15.071552	-0.050830	4.433408
250.860826	6736.931075	15.076557	-0.050839	4.430851
250.788604	6728.997158	15.081562	-0.050820	4.428328
250.736205	6720.945870	15.086567	-0.050805	4.425766
250.876089	6712.995430	15.091571	-0.050826	4.423236
250.686631	6704.971173	15.096576	-0.050785	4.420679
250.748466	6697.014393	15.101581	-0.050791	4.418143
250.625109	6689.004351	15.106586	-0.050763	4.415588
250.352972	6680.964164	15.111591	-0.050707	4.413021
250.157305	6672.969593	15.116595	-0.050665	4.410468
250.226648	6664.963761	15.121600	-0.050673	4.407910
250.250427	6656.981847	15.126605	-0.050672	4.405359
250.362454	6648.996275	15.131610	-0.050688	4.402806
250.303664	6640.982055	15.136615	-0.050671	4.400241
250.331330	6633.019821	15.141619	-0.050671	4.397691
250.177548	6624.974693	15.146624	-0.050637	4.395113
250.067199	6616.983261	15.151629	-0.050612	4.392550
250.081249	6608.973946	15.156634	-0.050609	4.389981
250.221666	6600.961264	15.161639	-0.050630	4.387410
250.313315	6592.952155	15.166643	-0.050642	4.384838
249.992959	6585.005633	15.171648	-0.050577	4.382283
249.948518	6576.986062	15.176653	-0.050563	4.379704
249.858672	6569.057447	15.181658	-0.050541	4.377153
249.999875	6560.954687	15.186663	-0.050562	4.374546
250.062901	6552.994804	15.191667	-0.050568	4.371982
249.885533	6544.944381	15.196672	-0.050530	4.369386
249.806427	6537.015984	15.201677	-0.050510	4.366829
249.889516	6528.997243	15.206682	-0.050520	4.364242
249.740085	6520.996474	15.211687	-0.050487	4.361658
249.766614	6512.999942	15.216691	-0.050487	4.359075
249.813987	6505.013525	15.221696	-0.050490	4.356494
249.886268	6496.954133	15.226701	-0.050499	4.353888
249.700041	6488.845003	15.231706	-0.050459	4.351262
249.388288	6480.895706	15.236711	-0.050395	4.348686
249.589046	6472.918490	15.241715	-0.050427	4.346102
249.610366	6464.913113	15.246720	-0.050426	4.343507
249.331064	6456.943873	15.251725	-0.050369	4.340920
249.371582	6448.977506	15.256730	-0.050371	4.338334
249.427649	6440.947321	15.261735	-0.050376	4.335726
249.453191	6432.933178	15.266739	-0.050376	4.333122
249.525649	6424.905550	15.271744	-0.050384	4.330512
249.489217	6416.933101	15.276749	-0.050372	4.327917
249.338358	6408.966083	15.281754	-0.050338	4.325322
249.417019	6400.970024	15.286759	-0.050348	4.322718
249.254201	6392.946885	15.291763	-0.050312	4.320102
249.243310	6384.982625	15.296768	-0.050305	4.317504
249.142203	6376.902842	15.301773	-0.050281	4.314866
249.345745	6368.946175	15.306778	-0.050313	4.312269
249.147641	6360.899518	15.311783	-0.050271	4.309638
249.113591	6352.935128	15.316787	-0.050259	4.307034
249.046228	6344.907683	15.321792	-0.050242	4.304407
249.111683	6336.957306	15.326797	-0.050249	4.301805
248.985144	6328.935375	15.331802	-0.050220	4.299176
248.891847	6320.967114	15.336807	-0.050197	4.296564
249.104663	6312.898207	15.341811	-0.050231	4.293919
249.072916	6304.889704	15.346816	-0.050220	4.291290
249.018637	6296.866731	15.351821	-0.050205	4.288655
248.775044	6288.912371	15.356826	-0.050154	4.286040
248.810332	6280.897999	15.361831	-0.050155	4.283405
248.877597	6272.909555	15.366835	-0.050163	4.280778
248.778627	6264.945444	15.371840	-0.050139	4.278155
248.711148	6256.921015	15.376845	-0.050121	4.275512
248.692864	6248.905982	15.381850	-0.050112	4.272870
248.794238	6240.857758	15.386855	-0.050126	4.270216
248.843659	6232.892488	15.391859	-0.050130	4.267588
248.578898	6224.893240	15.396864	-0.050075	4.264944
248.572957	6216.876994	15.401869	-0.050069	4.262296
248.808942	6208.910166	15.406874	-0.050108	4.259664
248.818441	6200.898690	15.411879	-0.050104	4.257014
248.651122	6192.926292	15.416883	-0.050068	4.254373
248.530690	6184.873763	15.421888	-0.050040	4.251705
248.376401	6176.883788	15.426893	-0.050006	4.249055
248.426533	6168.887486	15.431898	-0.050010	4.246404
248.233258	6160.905863	15.436903	-0.049969	4.243753
248.469464	6152.890783	15.441907	-0.050007	4.241094
248.529886	6144.933579	15.446912	-0.050013	4.238450
248.403469	6136.936957	15.451917	-0.049984	4.235790
248.511422	6128.955502	15.456922	-0.049999	4.233136
248.377247	6120.817337	15.461927	-0.049969	4.230425
248.332628	6112.908551	15.466931	-0.049955	4.227790
248.140042	6104.887378	15.471936	-0.049914	4.225115
248.123894	6096.935359	15.476941	-0.049906	4.222462
248.142347	6088.940557	15.481946	-0.049904	4.219794
247.883785	6080.966647	15.486951	-0.049851	4.217129
247.992203	6072.934445	15.491955	-0.049866	4.214446
247.971072	6064.916882	15.496960	-0.049856	4.211765
247.987554	6056.893956	15.501965	-0.049854	4.209080
248.000184	6048.946181	15.506970	-0.049851	4.206419
247.847370	6040.931270	15.511975	-0.049817	4.203733
247.885991	6032.952793	15.516979	-0.049819	4.201058
247.940141	6024.931449	15.521984	-0.049824	4.198368
247.947693	6016.914851	15.526989	-0.049820	4.195677
247.906568	6008.853850	15.531994	-0.049807	4.192969
247.834454	6000.821362	15.536999	-0.049789	4.190269
247.762704	5992.864604	15.542003	-0.049770	4.187592
247.870348	5984.858917	15.547008	-0.049785	4.184899
247.714490	5976.935544	15.552013	-0.049750	4.182229
247.588658	5968.876460	15.557018	-0.049722	4.179512
247.451286	5960.910987	15.562023	-0.049691	4.176824
247.620506	5952.902579	15.567027	-0.049717	4.174124
247.619431	5944.888353	15.572032	-0.049712	4.171418
247.649981	5936.850556	15.577037	-0.049712	4.168703
247.575891	5928.903698	15.582042	-0.049693	4.166016
247.316469	5920.890818	15.587047	-0.049639	4.163302
247.375722	5912.900946	15.592051	-0.049645	4.160598
247.286918	5904.913979	15.597056	-0.049623	4.157892
247.318812	5896.859019	15.602061	-0.049624	4.155162
247.372708	5888.887715	15.607066	-0.049629	4.152459
247.460322	5880.833967	15.612071	-0.049640	4.149726
247.446622	5872.856147	15.617075	-0.049632	4.147017
247.131690	5864.864832	15.622080	-0.049568	4.144297
247.273604	5856.888333	15.627085	-0.049589	4.141586
247.303419	5848.910931	15.632090	-0.049589	4.138872
246.963447	5840.895237	15.637095	-0.049521	4.136138
247.047671	5832.911776	15.642099	-0.049531	4.133419
246.942955	5824.852542	15.647104	-0.049506	4.130670
246.974731	5816.861424	15.652109	-0.049507	4.127944
246.818576	5808.887971	15.657114	-0.049473	4.125220
246.813438	5800.896921	15.662119	-0.049466	4.122489
246.888273	5792.893596	15.667123	-0.049475	4.119754
246.786656	5784.922223	15.672128	-0.049451	4.117026
246.900386	5776.884283	15.677133	-0.049467	4.114276
246.928431	5768.851267	15.682138	-0.049467	4.111524
246.804851	5760.837567	15.687143	-0.049438	4.108776
246.709789	5752.864596	15.692147	-0.049415	4.106040
246.577753	5744.863851	15.697152	-0.049385	4.103292
246.515585	5736.886737	15.702157	-0.049369	4.100551
246.568001	5728.911463	15.707162	-0.049373	4.097810
246.595811	5720.870782	15.712167	-0.049373	4.095045
246.595144	5712.881981	15.717171	-0.049367	4.092296
246.361255	5704.872376	15.722176	-0.049319	4.089534
246.467854	5696.888353	15.727181	-0.049333	4.086784
246.541100	5688.920040	15.732186	-0.049342	4.084037
246.447489	5680.936585	15.737191	-0.049319	4.081280
246.324592	5672.937149	15.742195	-0.049291	4.078516
246.255213	5664.939236	15.747200	-0.049272	4.075751
246.317327	5656.918004	15.752205	-0.049279	4.072978
246.211521	5648.900921	15.757210	-0.049254	4.070202
246.028433	5640.897921	15.762215	-0.049214	4.067428
246.057536	5632.891762	15.767219	-0.049214	4.064655
245.993534	5624.944401	15.772224	-0.049197	4.061898
245.999980	5616.922203	15.777229	-0.049193	4.059114
246.215996	5608.979486	15.782234	-0.049228	4.056359
245.997970	5600.921001	15.787239	-0.049182	4.053556
245.889185	5592.894119	15.792243	-0.049157	4.050764
245.975203	5584.899591	15.797248	-0.049167	4.047983
245.889683	5576.902558	15.802253	-0.049146	4.045197
245.940545	5568.944683	15.807258	-0.049150	4.042425
245.793690	5560.904036	15.812263	-0.049118	4.039620
246.078285	5552.971268	15.817267	-0.049166	4.036856
245.912268	5544.911305	15.822272	-0.049129	4.034039
245.763385	5536.783957	15.827277	-0.049096	4.031197
245.896091	5528.848306	15.832282	-0.049116	4.028425
245.637221	5520.857591	15.837287	-0.049062	4.025625
245.564609	5512.915177	15.842291	-0.049043	4.022843
245.634174	5504.913235	15.847296	-0.049051	4.020040
245.768087	5496.902429	15.852301	-0.049071	4.017234
245.592717	5488.894924	15.857306	-0.049033	4.014421
245.539602	5480.876093	15.862311	-0.049018	4.011605
245.464369	5472.866580	15.867315	-0.048998	4.008789
245.317924	5464.903223	15.872320	-0.048966	4.005987
245.257554	5456.883955	15.877325	-0.048949	4.003165
245.380583	5448.906356	15.882330	-0.048967	4.000358
245.338960	5440.927658	15.887335	-0.048954	3.997546
245.244347	5432.901267	15.892339	-0.048931	3.994714
245.403747	5424.883954	15.897344	-0.048955	3.991888
245.382466	5416.871775	15.902349	-0.048946	3.989058
245.393190	5408.907090	15.907354	-0.048943	3.986244
245.240894	5400.893851	15.912359	-0.048909	3.983408
245.077874	5392.898357	15.917363	-0.048873	3.980576
245.174590	5384.938723	15.922368	-0.048886	3.977759
244.828191	5376.925466	15.927373	-0.048816	3.974914
244.992816	5368.912360	15.932378	-0.048842	3.972075
244.953361	5360.882974	15.937383	-0.048829	3.969225
244.998933	5352.939681	15.942387	-0.048832	3.966405
244.846057	5344.935145	15.947392	-0.048799	3.963557
244.855465	5336.934758	15.952397	-0.048795	3.960712
244.924686	5329.016153	15.957402	-0.048803	3.957895
244.680131	5320.962419	15.962407	-0.048752	3.955023
244.727700	5312.927551	15.967411	-0.048755	3.952160
244.923889	5304.900843	15.972416	-0.048787	3.949300
244.746121	5296.934973	15.977421	-0.048748	3.946454
244.682548	5288.924737	15.982426	-0.048731	3.943592
244.782754	5280.941052	15.987431	-0.048744	3.940740
244.809066	5272.991215	15.992435	-0.048744	3.937897
244.610638	5264.977251	15.997440	-0.048702	3.935024
244.541132	5256.940990	16.002445	-0.048684	3.932144
244.421431	5248.971505	16.007450	-0.048656	3.929285
244.299492	5240.967976	16.012455	-0.048628	3.926412
244.435993	5232.973781	16.017459	-0.048648	3.923544
244.293390	5224.968309	16.022464	-0.048616	3.920665
244.299703	5216.983748	16.027469	-0.048612	3.917795
244.334607	5208.989699	16.032474	-0.048613	3.914919
244.168870	5200.991906	16.037479	-0.048577	3.912036
244.295092	5192.970282	16.042483	-0.048596	3.909148
244.089554	5184.989050	16.047488	-0.048552	3.906266
244.196307	5176.938743	16.052493	-0.048567	3.903363
244.445519	5168.957808	16.057498	-0.048608	3.900485
244.023638	5161.005757	16.062503	-0.048524	3.897603
244.004787	5152.995423	16.067507	-0.048515	3.894706
244.192492	5144.952564	16.072512	-0.048545	3.891798
244.125724	5136.927408	16.077517	-0.048527	3.888890
244.088469	5128.995399	16.082522	-0.048515	3.886014
243.920148	5120.957560	16.087527	-0.048478	3.883095
243.925491	5113.003363	16.092531	-0.048474	3.880208
243.832464	5105.032894	16.097536	-0.048451	3.877310
243.811749	5096.970964	16.102541	-0.048442	3.874379
243.793006	5088.742648	16.107546	-0.048433	3.871384
243.748506	5080.807508	16.112551	-0.048420	3.868494
243.714361	5072.870052	16.117555	-0.048408	3.865601
243.907872	5064.920106	16.122560	-0.048439	3.862705
243.647559	5056.930003	16.127565	-0.048385	3.859784
243.590300	5048.994685	16.132570	-0.048369	3.856885
243.593316	5040.979209	16.137575	-0.048364	3.853955
243.589720	5032.959110	16.142579	-0.048358	3.851021
243.523048	5024.988714	16.147584	-0.048341	3.848102
243.342635	5016.962611	16.152589	-0.048302	3.845158
243.484511	5008.997011	16.157594	-0.048323	3.842241
243.355495	5001.009278	16.162599	-0.048294	3.839307
243.265805	4993.050988	16.167603	-0.048272	3.836383
243.321615	4985.064237	16.172608	-0.048277	3.833449
243.258426	4976.989366	16.177613	-0.048260	3.830478
243.258967	4969.037566	16.182618	-0.048255	3.827552
243.261930	4960.969704	16.187623	-0.048250	3.824580
243.358098	4953.054312	16.192627	-0.048262	3.821665
243.371721	4945.054932	16.197632	-0.048260	3.818714
243.340297	4937.028838	16.202637	-0.048249	3.815750
243.286259	4929.093935	16.207642	-0.048233	3.812818
243.061224	4921.017292	16.212647	-0.048186	3.809826
242.971614	4913.073278	16.217651	-0.048164	3.806885
243.009255	4905.060574	16.222656	-0.048166	3.803918
242.865395	4897.084994	16.227661	-0.048134	3.800959
242.945042	4889.106714	16.232666	-0.048143	3.798002
242.862582	4881.073595	16.237671	-0.048123	3.795018
242.854432	4873.029821	16.242675	-0.048116	3.792030
242.830381	4865.052944	16.247680	-0.048106	3.789064
242.860742	4857.001913	16.252685	-0.048106	3.786069
242.839580	4849.105325	16.257690	-0.048097	3.783128
242.745586	4841.051789	16.262695	-0.048074	3.780124
242.574321	4833.106428	16.267699	-0.048037	3.777157
242.786251	4825.036333	16.272704	-0.048071	3.774150
242.827602	4817.041426	16.277709	-0.048074	3.771164
242.492101	4809.073299	16.282714	-0.048006	3.768178
242.534313	4801.034335	16.287719	-0.048009	3.765171
242.504462	4793.120381	16.292723	-0.047998	3.762207
242.351911	4785.090319	16.297728	-0.047964	3.759194
242.280526	4777.119173	16.302733	-0.047946	3.756203
242.412409	4769.081967	16.307738	-0.047965	3.753189
242.467178	4761.048478	16.312743	-0.047970	3.750173
242.499811	4753.051868	16.317747	-0.047970	3.747167
242.284353	4745.038184	16.322752	-0.047925	3.744147
242.541822	4737.115795	16.327757	-0.047968	3.741170
242.461576	4729.138856	16.332762	-0.047948	3.738162
242.169274	4721.111420	16.337767	-0.047888	3.735127
242.147088	4713.133083	16.342771	-0.047878	3.732115
242.077571	4705.114640	16.347776	-0.047860	3.729084
241.838241	4697.132546	16.352781	-0.047810	3.726061
242.094302	4689.148511	16.357786	-0.047853	3.723046
241.933844	4681.176905	16.362791	-0.047818	3.720023
241.808107	4673.195627	16.367795	-0.047789	3.716995
241.927164	4665.125343	16.372800	-0.047806	3.713937
242.044030	4657.037140	16.377805	-0.047822	3.710869
241.949641	4649.096582	16.382810	-0.047799	3.707850
241.845891	4641.090927	16.387815	-0.047775	3.704803
241.908888	4633.161401	16.392819	-0.047781	3.701787
241.879600	4625.168970	16.397824	-0.047770	3.698742
241.653658	4617.164108	16.402829	-0.047723	3.695685
241.865206	4609.187916	16.407834	-0.047757	3.692647
241.621931	4601.142770	16.412839	-0.047707	3.689569
241.546769	4593.202757	16.417843	-0.047687	3.686533
241.537387	4585.189077	16.422848	-0.047680	3.683468
241.498483	4577.204424	16.427853	-0.047668	3.680410
241.495206	4569.235456	16.432858	-0.047662	3.677357
241.392088	4561.221194	16.437863	-0.047637	3.674282
241.393439	4553.202615	16.442867	-0.047632	3.671205
241.260332	4545.216068	16.447872	-0.047602	3.668134
241.090571	4537.177858	16.452877	-0.047565	3.665040
241.243123	4529.230960	16.457882	-0.047588	3.661986
241.174336	4521.198672	16.462887	-0.047570	3.658892
241.147044	4513.249752	16.467891	-0.047560	3.655828
240.969499	4505.249806	16.472896	-0.047522	3.652738
241.086272	4497.180780	16.477901	-0.047538	3.649626
241.016654	4489.243666	16.482906	-0.047520	3.646558
240.921649	4481.254487	16.487911	-0.047497	3.643466
240.968049	4473.261567	16.492915	-0.047500	3.640374
240.984497	4465.300863	16.497920	-0.047498	3.637291
240.902842	4457.269998	16.502925	-0.047478	3.634176
241.150335	4449.203839	16.507930	-0.047518	3.631053
241.069054	4441.215690	16.512935	-0.047498	3.627949
240.929223	4433.226476	16.517939	-0.047467	3.624840
240.871725	4425.284934	16.522944	-0.047451	3.621749
240.807616	4417.263298	16.527949	-0.047433	3.618624
240.844101	4409.266351	16.532954	-0.047435	3.615509
240.738843	4401.279919	16.537959	-0.047410	3.612391
240.784471	4393.268138	16.542963	-0.047413	3.609265
240.845545	4385.289342	16.547968	-0.047419	3.606150
240.818722	4377.288578	16.552973	-0.047409	3.603021
240.810307	4369.320577	16.557978	-0.047402	3.599902
240.655462	4361.362030	16.562983	-0.047368	3.596780
240.648228	4353.356067	16.567987	-0.047361	3.593641
240.673183	4345.315020	16.572992	-0.047361	3.590487
240.802449	4337.321960	16.577997	-0.047380	3.587352
240.764739	4329.332862	16.583002	-0.047367	3.584210
240.451161	4321.396237	16.588007	-0.047304	3.581079
240.622093	4313.392537	16.593011	-0.047330	3.577932
240.570553	4305.380400	16.598016	-0.047315	3.574773
240.328870	4297.374283	16.603021	-0.047265	3.571608
240.531004	4289.378325	16.608026	-0.047297	3.568457
240.266070	4281.368485	16.613031	-0.047243	3.565284
240.167724	4273.420657	16.618035	-0.047219	3.562138
240.173670	4265.428818	16.623040	-0.047215	3.558974
240.147768	4257.411800	16.628045	-0.047205	3.555797
240.253036	4249.359147	16.633050	-0.047219	3.552606
240.266931	4241.296923	16.638055	-0.047216	3.549407
240.139398	4233.342099	16.643059	-0.047187	3.546243
240.205152	4225.373654	16.648064	-0.047194	3.543076
239.763840	4217.389304	16.653069	-0.047107	3.539885
239.873470	4209.422501	16.658074	-0.047122	3.536715
239.893623	4201.391299	16.663079	-0.047120	3.533513
240.181138	4193.365086	16.668083	-0.047169	3.530318
239.881997	4185.457792	16.673088	-0.047108	3.527151
239.795469	4177.411973	16.678093	-0.047086	3.523931
239.934712	4169.457678	16.683098	-0.047107	3.520753
239.848511	4161.452982	16.688103	-0.047086	3.517544
239.631009	4153.484399	16.693107	-0.047040	3.514343
239.807536	4145.439189	16.698112	-0.047067	3.511120
239.644526	4137.463234	16.703117	-0.047032	3.507911
239.635759	4129.483500	16.708122	-0.047025	3.504703
239.759134	4121.489200	16.713127	-0.047043	3.501490
239.811147	4113.494563	16.718131	-0.047047	3.498272
239.671602	4105.536129	16.723136	-0.047016	3.495060
239.661439	4097.528568	16.728141	-0.047009	3.491828
239.775852	4089.534897	16.733146	-0.047025	3.488604
239.287662	4081.553432	16.738151	-0.046928	3.485362
239.293064	4073.582415	16.743155	-0.046924	3.482137
239.374079	4065.595096	16.748160	-0.046934	3.478904
239.308520	4057.583654	16.753165	-0.046916	3.475655
239.471571	4049.548538	16.758170	-0.046942	3.472400
239.319111	4041.507548	16.763175	-0.046908	3.469129
239.400313	4033.541574	16.768179	-0.046918	3.465893
239.288401	4025.570055	16.773184	-0.046892	3.462646
239.228226	4017.569748	16.778189	-0.046875	3.459386
239.267188	4009.621112	16.783194	-0.046877	3.456147
239.264030	4001.573178	16.788199	-0.046871	3.452863
239.043708	3993.579455	16.793203	-0.046825	3.449591
238.937824	3985.614705	16.798208	-0.046800	3.446331
238.755877	3977.614903	16.803213	-0.046761	3.443051
238.758720	3969.641324	16.808218	-0.046756	3.439785
238.819628	3961.665266	16.813223	-0.046762	3.436517
238.796573	3953.628346	16.818227	-0.046752	3.433218
238.877341	3945.621820	16.823232	-0.046762	3.429932
238.693543	3937.619585	16.828237	-0.046723	3.426636
238.810090	3929.630023	16.833242	-0.046739	3.423351
238.767760	3921.643748	16.838247	-0.046726	3.420060
238.733724	3913.690230	16.843251	-0.046714	3.416779
238.733495	3905.696213	16.848256	-0.046709	3.413479
238.438774	3897.656573	16.853261	-0.046649	3.410147
238.285161	3889.720340	16.858266	-0.046615	3.406860
238.271502	3881.716106	16.863271	-0.046607	3.403546
238.411486	3873.736965	16.868275	-0.046628	3.400244
238.306125	3865.780039	16.873280	-0.046603	3.396940
238.249677	3857.702792	16.878285	-0.046587	3.393585
238.202997	3849.679296	16.883290	-0.046573	3.390249
238.194207	3841.691283	16.888295	-0.046566	3.386925
238.201851	3833.730714	16.893299	-0.046562	3.383611
238.269721	3825.771347	16.898304	-0.046570	3.380295
238.216767	3817.796364	16.903309	-0.046555	3.376966
238.284664	3809.807037	16.908314	-0.046562	3.373632
238.093992	3801.777472	16.913319	-0.046521	3.370268
238.018907	3793.785657	16.918323	-0.046502	3.366921
237.786783	3785.840611	16.923328	-0.046454	3.363584
237.805194	3777.820282	16.928333	-0.046452	3.360222
237.998694	3769.858332	16.933338	-0.046482	3.356887
237.741574	3761.839097	16.938343	-0.046429	3.353509
237.739979	3753.816368	16.943347	-0.046424	3.350134
237.897693	3745.839067	16.948352	-0.046448	3.346782
237.675899	3737.861920	16.953357	-0.046401	3.343412
237.651705	3729.873509	16.958362	-0.046391	3.340041
237.498372	3721.917004	16.963367	-0.046358	3.336675
237.879170	3713.863596	16.968371	-0.046423	3.333285
237.741016	3705.889479	16.973376	-0.046392	3.329906
237.572904	3697.904055	16.978381	-0.046356	3.326517
237.610653	3689.920515	16.983386	-0.046357	3.323134
237.477431	3681.921939	16.988391	-0.046327	3.319734
237.314965	3673.977541	16.993395	-0.046292	3.316352
237.305714	3665.963926	16.998400	-0.046285	3.312944
237.326533	3657.899463	17.003405	-0.046283	3.309511
237.117305	3649.984634	17.008410	-0.046239	3.306130
237.123012	3641.963760	17.013415	-0.046235	3.302708
237.459967	3633.951561	17.018419	-0.046292	3.299299
237.410911	3626.022923	17.023424	-0.046278	3.295908
237.116654	3618.007812	17.028429	-0.046218	3.292467
237.247579	3609.997227	17.033434	-0.046237	3.289040
237.089782	3602.028953	17.038439	-0.046202	3.285617
237.079058	3594.054329	17.043443	-0.046195	3.282193
237.181075	3586.077106	17.048448	-0.046209	3.278768
237.166160	3578.072354	17.053453	-0.046201	3.275324
237.231958	3570.061453	17.058458	-0.046208	3.271877
237.115311	3562.065450	17.063463	-0.046181	3.268425
237.137258	3554.060244	17.068467	-0.046179	3.264971
237.106355	3546.117450	17.073472	-0.046168	3.261539
236.725956	3538.132820	17.078477	-0.046092	3.258070
236.961467	3530.129136	17.083482	-0.046131	3.254615
236.907556	3522.128085	17.088487	-0.046115	3.251145
236.790892	3514.144270	17.093491	-0.046088	3.247676
236.615404	3506.162988	17.098496	-0.046051	3.244203
236.668419	3498.181377	17.103501	-0.046055	3.240735
236.739123	3490.205930	17.108506	-0.046063	3.237266
236.623351	3482.206933	17.113511	-0.046036	3.233776
236.654086	3474.123574	17.118515	-0.046037	3.230251
236.539069	3466.178398	17.123520	-0.046010	3.226777
236.383080	3458.194994	17.128525	-0.045976	3.223281
236.478350	3450.206749	17.133530	-0.045988	3.219789
236.361449	3442.245643	17.138535	-0.045961	3.216296
236.477633	3434.232877	17.143539	-0.045977	3.212787
236.390078	3426.240931	17.148544	-0.045956	3.209274
236.525709	3418.248037	17.153549	-0.045976	3.205767
236.394662	3410.316751	17.158554	-0.045946	3.202271
236.249172	3402.335354	17.163559	-0.045914	3.198749
236.080148	3394.341004	17.168563	-0.045877	3.195217
236.381344	3386.290967	17.173568	-0.045928	3.191675
236.202833	3378.312486	17.178573	-0.045889	3.188142
236.005055	3370.329977	17.183578	-0.045847	3.184601
236.234416	3362.354222	17.188583	-0.045885	3.181078
236.156048	3354.364698	17.193587	-0.045865	3.177532
236.299067	3346.357195	17.198592	-0.045886	3.173983
235.942931	3338.386382	17.203597	-0.045814	3.170425
236.030617	3330.409136	17.208602	-0.045825	3.166880
235.751495	3322.433590	17.213607	-0.045768	3.163315
235.742974	3314.450704	17.218611	-0.045761	3.159755
235.897787	3306.479108	17.223616	-0.045785	3.156202
235.734737	3298.439882	17.228621	-0.045749	3.152602
235.823280	3290.434865	17.233626	-0.045760	3.149024
235.835484	3282.436623	17.238631	-0.045757	3.145441
235.721282	3274.482842	17.243635	-0.045731	3.141869
235.595788	3266.529546	17.248640	-0.045702	3.138293
235.616971	3258.518193	17.253645	-0.045701	3.134692
235.601294	3250.543937	17.258650	-0.045693	3.131103
235.673123	3242.531409	17.263655	-0.045701	3.127496
235.548503	3234.545463	17.268659	-0.045672	3.123888
235.680437	3226.583435	17.273664	-0.045692	3.120299
235.437568	3218.624277	17.278669	-0.045641	3.116689
235.469768	3210.609160	17.283674	-0.045642	3.113063
235.454965	3202.587402	17.288679	-0.045634	3.109427
235.487130	3194.597164	17.293683	-0.045634	3.105803
235.506682	3186.662838	17.298688	-0.045633	3.102200
235.476821	3178.661719	17.303693	-0.045622	3.098560
235.590252	3170.664523	17.308698	-0.045638	3.094924
235.210107	3162.696955	17.313703	-0.045562	3.091275
235.269151	3154.669368	17.318707	-0.045568	3.087614
235.193042	3146.722987	17.323712	-0.045548	3.083980
235.044532	3138.758562	17.328717	-0.045515	3.080330
235.174826	3130.778763	17.333722	-0.045534	3.076681
235.010477	3122.736264	17.338727	-0.045498	3.072985
234.971724	3114.671019	17.343731	-0.045486	3.069281
234.851408	3106.742652	17.348736	-0.045458	3.065631
234.889674	3098.753330	17.353741	-0.045460	3.061956
234.982998	3090.782162	17.358746	-0.045472	3.058288
234.801557	3082.810169	17.363751	-0.045433	3.054601
234.821328	3074.798148	17.368755	-0.045431	3.050902
234.962997	3066.839280	17.373760	-0.045452	3.047228
234.705648	3058.870482	17.378765	-0.045399	3.043526
234.707243	3050.894153	17.383770	-0.045394	3.039829
234.630943	3042.927535	17.388775	-0.045375	3.036128
234.717531	3034.889974	17.393779	-0.045386	3.032397
234.763171	3026.919500	17.398784	-0.045389	3.028691
234.635143	3018.933991	17.403789	-0.045360	3.024965
234.492814	3011.007379	17.408794	-0.045328	3.021261
234.446207	3002.993025	17.413799	-0.045314	3.017516
234.542599	2994.983671	17.418803	-0.045327	3.013776
234.566139	2986.995192	17.423808	-0.045326	3.010037
234.254753	2979.023230	17.428813	-0.045263	3.006285
234.175732	2971.070805	17.433818	-0.045243	3.002549
234.193849	2963.089516	17.438823	-0.045241	2.998800
234.336299	2955.079854	17.443827	-0.045262	2.995038
234.314030	2947.080413	17.448832	-0.045252	2.991269
234.187516	2939.088903	17.453837	-0.045224	2.987493
234.112785	2931.123198	17.458842	-0.045204	2.983727
234.021530	2923.140318	17.463847	-0.045182	2.979948
234.007058	2915.173919	17.468851	-0.045174	2.976175
234.090975	2907.165650	17.473856	-0.045185	2.972383
234.029830	2899.158118	17.478861	-0.045168	2.968579
234.058758	2891.194545	17.483866	-0.045168	2.964795
233.968081	2883.248734	17.488871	-0.045146	2.961009
233.936596	2875.270096	17.493875	-0.045135	2.957206
234.016725	2867.274006	17.498880	-0.045144	2.953395
233.721550	2859.273896	17.503885	-0.045084	2.949557
233.729490	2851.303716	17.508890	-0.045080	2.945745
233.562910	2843.352356	17.513895	-0.045044	2.941928
233.514363	2835.353044	17.518899	-0.045030	2.938089
233.610758	2827.380274	17.523904	-0.045042	2.934265
233.399718	2819.376753	17.528909	-0.044998	2.930405
233.594292	2811.384944	17.533914	-0.045029	2.926567
233.579664	2803.417994	17.538919	-0.045021	2.922725
233.473080	2795.458683	17.543923	-0.044996	2.918877
233.653521	2787.455175	17.548928	-0.045024	2.915018
233.365137	2779.393855	17.553933	-0.044965	2.911100
233.438491	2771.424693	17.558938	-0.044973	2.907241
233.456329	2763.448417	17.563943	-0.044971	2.903371
233.262818	2755.504211	17.568947	-0.044930	2.899500
233.346013	2747.545199	17.573952	-0.044940	2.895631
233.374260	2739.521565	17.578957	-0.044940	2.891722
233.134031	2731.564182	17.583962	-0.044890	2.887827
233.080295	2723.587962	17.588967	-0.044875	2.883926
233.045460	2715.615991	17.593971	-0.044863	2.880024
233.245198	2707.645828	17.598976	-0.044895	2.876130
233.121112	2699.641835	17.603981	-0.044867	2.872196
233.192614	2691.647902	17.608986	-0.044875	2.868272
233.100094	2683.652216	17.613991	-0.044852	2.864334
232.854210	2675.731062	17.618995	-0.044801	2.860418
233.087591	2667.752332	17.624000	-0.044839	2.856495
233.017346	2659.747348	17.629005	-0.044821	2.852536
232.828856	2651.783282	17.634010	-0.044781	2.848586
232.694642	2643.821068	17.639015	-0.044750	2.844634
232.697936	2635.875773	17.644019	-0.044746	2.840693
232.716632	2627.901441	17.649024	-0.044744	2.836733
232.444417	2619.876028	17.654029	-0.044688	2.832725
232.545292	2611.873431	17.659034	-0.044702	2.828744
232.454940	2603.879499	17.664039	-0.044679	2.824751
232.346249	2595.923374	17.669043	-0.044654	2.820770
232.396454	2587.943489	17.674048	-0.044658	2.816781
232.406506	2579.931542	17.679053	-0.044655	2.812768
232.468623	2571.961723	17.684058	-0.044661	2.808773
232.096300	2564.027177	17.689063	-0.044586	2.804765
232.151553	2556.049877	17.694067	-0.044591	2.800754
232.140525	2548.087299	17.699072	-0.044584	2.796741
232.172071	2540.071871	17.704077	-0.044585	2.792699
232.202050	2532.077473	17.709082	-0.044585	2.788661
232.242405	2524.097748	17.714087	-0.044587	2.784625
232.110603	2516.164989	17.719091	-0.044557	2.780597
232.114477	2508.204012	17.724096	-0.044553	2.776557
231.965880	2500.204286	17.729101	-0.044520	2.772482
232.029297	2492.207547	17.734106	-0.044526	2.768415
232.008352	2484.248927	17.739111	-0.044517	2.764357
232.138009	2476.271504	17.744115	-0.044536	2.760292
232.130027	2468.321932	17.749120	-0.044529	2.756227
231.800638	2460.291535	17.754125	-0.044463	2.752096
231.688277	2452.290989	17.759130	-0.044436	2.747986
231.697153	2444.322780	17.764135	-0.044433	2.743894
231.740864	2436.342314	17.769139	-0.044436	2.739792
231.724943	2428.408092	17.774144	-0.044427	2.735704
231.657792	2420.402317	17.779149	-0.044410	2.731570
231.695452	2412.421600	17.784154	-0.044411	2.727449
231.543124	2404.455043	17.789159	-0.044378	2.723318
231.372130	2396.507100	17.794163	-0.044341	2.719188
231.511515	2388.542068	17.799168	-0.044361	2.715063
231.371707	2380.539042	17.804173	-0.044330	2.710894
231.233122	2372.575821	17.809178	-0.044299	2.706739
231.222388	2364.604174	17.814183	-0.044292	2.702582
231.398692	2356.615145	17.819187	-0.044319	2.698421
231.113226	2348.685584	17.824192	-0.044261	2.694256
231.148659	2340.667218	17.829197	-0.044262	2.690058
231.261942	2332.697133	17.834202	-0.044278	2.685883
230.998138	2324.783803	17.839207	-0.044224	2.681708
231.013291	2316.788685	17.844211	-0.044221	2.677501
231.051228	2308.811050	17.849216	-0.044223	2.673298
230.924769	2300.789108	17.854221	-0.044194	2.669055
230.885170	2292.830769	17.859226	-0.044181	2.664844
230.885050	2284.865492	17.864231	-0.044176	2.660625
230.902525	2276.903051	17.869235	-0.044174	2.656402
230.965783	2268.914193	17.874240	-0.044181	2.652162
230.857022	2260.940391	17.879245	-0.044155	2.647911
230.861137	2252.962968	17.884250	-0.044151	2.643659
230.650885	2245.033778	17.889255	-0.044106	2.639412
230.599690	2237.080098	17.894259	-0.044091	2.635155
230.634313	2229.061157	17.899264	-0.044093	2.630862
230.528463	2221.101700	17.904269	-0.044068	2.626585
230.496521	2213.141193	17.909274	-0.044056	2.622305
230.588435	2205.168792	17.914279	-0.044068	2.618020
230.525602	2197.194158	17.919283	-0.044051	2.613716
230.336486	2189.221813	17.924288	-0.044011	2.609398
230.225357	2181.266042	17.929293	-0.043985	2.605087
230.252398	2173.310023	17.934298	-0.043985	2.600778
230.032607	2165.374129	17.939303	-0.043938	2.596456
230.188052	2157.237113	17.944307	-0.043962	2.592043
230.186221	2149.221764	17.949312	-0.043956	2.587678
230.015448	2141.278009	17.954317	-0.043919	2.583333
229.904120	2133.371649	17.959322	-0.043893	2.579006
229.887015	2125.416329	17.964327	-0.043885	2.574650
229.897887	2117.439090	17.969331	-0.043882	2.570277
229.870064	2109.484558	17.974336	-0.043871	2.565907
229.971983	2101.505365	17.979341	-0.043885	2.561524
229.970518	2093.565299	17.984346	-0.043879	2.557149
229.762218	2085.617289	17.989351	-0.043835	2.552747
229.827076	2077.620227	17.994355	-0.043842	2.548329
229.912300	2069.665370	17.999360	-0.043853	2.543929
229.502882	2061.730430	18.004365	-0.043771	2.539497
229.557282	2053.772321	18.009370	-0.043776	2.535077
229.605547	2045.763015	18.014375	-0.043780	2.530620
229.485310	2037.804715	18.019379	-0.043752	2.526172
229.411477	2029.870463	18.024384	-0.043733	2.521733
229.439847	2021.890581	18.029389	-0.043733	2.517268
229.304273	2013.927545	18.034394	-0.043703	2.512793
229.475650	2005.912901	18.039399	-0.043729	2.508303
229.391208	1997.948514	18.044403	-0.043708	2.503814
229.311490	1990.026613	18.049408	-0.043688	2.499342
229.319344	1982.047144	18.054413	-0.043684	2.494836
229.236895	1974.086054	18.059418	-0.043664	2.490325
229.253270	1966.104887	18.064423	-0.043662	2.485802
229.000524	1958.194318	18.069427	-0.043609	2.481290
229.113741	1950.232059	18.074432	-0.043625	2.476769
229.004726	1942.248630	18.079437	-0.043600	2.472210
229.210650	1934.243831	18.084442	-0.043633	2.467654
228.936717	1926.320168	18.089447	-0.043576	2.463101
228.757975	1918.385267	18.094451	-0.043538	2.458539
228.955888	1910.393859	18.099456	-0.043569	2.453965
228.982972	1902.399510	18.104461	-0.043569	2.449368
228.811608	1894.478685	18.109466	-0.043532	2.444790
228.468355	1886.565976	18.114471	-0.043463	2.440194
228.727924	1878.567660	18.119475	-0.043506	2.435586
228.812890	1870.529324	18.124480	-0.043516	2.430933
228.454721	1862.578034	18.129485	-0.043445	2.426288
228.634091	1854.603752	18.134490	-0.043473	2.421662
228.632807	1846.663981	18.139495	-0.043467	2.417033
228.369194	1838.729644	18.144499	-0.043413	2.412378
228.620223	1830.738647	18.149504	-0.043454	2.407720
228.577670	1822.774628	18.154509	-0.043441	2.403047
228.237520	1814.884902	18.159514	-0.043373	2.398385
228.214648	1806.934198	18.164519	-0.043363	2.393703
228.256070	1798.926478	18.169523	-0.043365	2.388983
228.319063	1790.972033	18.174528	-0.043372	2.384287
227.954999	1783.050699	18.179533	-0.043299	2.379567
228.092281	1775.091663	18.184538	-0.043319	2.374855
228.225825	1767.089022	18.189543	-0.043339	2.370108
227.967152	1759.157746	18.194547	-0.043285	2.365363
227.889938	1751.231663	18.199552	-0.043266	2.360625
227.902699	1743.276272	18.204557	-0.043263	2.355868
227.859213	1735.283132	18.209562	-0.043249	2.351074
227.901906	1727.305291	18.214567	-0.043252	2.346286
227.866874	1719.348275	18.219571	-0.043240	2.341495
227.788003	1711.431356	18.224576	-0.043220	2.336714
227.732864	1703.444355	18.229581	-0.043205	2.331883
227.701702	1695.493328	18.234586	-0.043194	2.327066
227.718823	1687.542168	18.239591	-0.043192	2.322243
227.662346	1679.608066	18.244595	-0.043176	2.317414
227.734061	1671.665575	18.249600	-0.043184	2.312580
227.672683	1663.687115	18.254605	-0.043167	2.307704
227.528092	1655.744607	18.259610	-0.043135	2.302832
227.462409	1647.817057	18.264615	-0.043118	2.297965
227.410037	1639.844108	18.269619	-0.043103	2.293061
227.444638	1631.887906	18.274624	-0.043104	2.288165
227.256663	1623.952613	18.279629	-0.043064	2.283252
227.317005	1616.007028	18.284634	-0.043070	2.278343
227.434478	1608.022561	18.289639	-0.043086	2.273404
227.131476	1600.031995	18.294643	-0.043025	2.268415
227.123078	1592.096500	18.299648	-0.043018	2.263474
227.268640	1584.129450	18.304653	-0.043040	2.258516
227.222667	1576.210656	18.309658	-0.043026	2.253561
227.140724	1568.243390	18.314663	-0.043005	2.248561
227.107545	1560.295776	18.319667	-0.042994	2.243567
227.200345	1552.369581	18.324672	-0.043006	2.238586
226.921184	1544.449931	18.329677	-0.042949	2.233565
226.766796	1536.510822	18.334682	-0.042915	2.228532
226.696619	1528.568585	18.339687	-0.042896	2.223493
226.664149	1520.616999	18.344691	-0.042885	2.218440
226.799378	1512.656775	18.349696	-0.042905	2.213384
226.563136	1504.709256	18.354701	-0.042856	2.208292
226.618984	1496.760251	18.359706	-0.042861	2.203214
226.450634	1488.858009	18.364711	-0.042824	2.198133
226.546588	1480.876349	18.369715	-0.042837	2.193014
226.594925	1472.902794	18.374720	-0.042841	2.187883
226.567369	1464.950436	18.379725	-0.042830	2.182747
226.528096	1457.033643	18.384730	-0.042818	2.177621
226.494788	1449.089459	18.389735	-0.042806	2.172466
226.286180	1441.154553	18.394739	-0.042762	2.167288
226.169229	1433.252717	18.399744	-0.042735	2.162128
226.165530	1425.288490	18.404749	-0.042729	2.156925
226.202152	1417.342227	18.409754	-0.042731	2.151725
226.192316	1409.394459	18.414759	-0.042724	2.146507
225.948426	1401.472768	18.419763	-0.042673	2.141272
226.137963	1393.539152	18.424768	-0.042703	2.136057
225.985042	1385.592136	18.429773	-0.042669	2.130787
225.819059	1377.672396	18.434778	-0.042633	2.125522
225.793157	1369.741648	18.439783	-0.042623	2.120249
225.875251	1361.786498	18.444787	-0.042633	2.114958
225.775132	1353.787620	18.449792	-0.042609	2.109606
225.620655	1345.862361	18.454797	-0.042575	2.104285
225.862523	1337.910066	18.459802	-0.042615	2.098970
225.734195	1330.002896	18.464807	-0.042586	2.093636
225.458589	1322.077950	18.469811	-0.042529	2.088263
225.717101	1314.115985	18.474816	-0.042572	2.082903
225.558319	1306.223096	18.479821	-0.042537	2.077534
225.603889	1298.276664	18.484826	-0.042541	2.072136
225.487376	1290.358305	18.489831	-0.042514	2.066726
225.318425	1282.440355	18.494835	-0.042477	2.061298
225.332291	1274.525031	18.499840	-0.042474	2.055875
225.236803	1266.572620	18.504845	-0.042451	2.050401
225.376676	1258.625288	18.509850	-0.042472	2.044940
225.131445	1250.749769	18.514855	-0.042421	2.039475
225.036832	1242.828356	18.519859	-0.042398	2.033978
225.160530	1234.846641	18.524864	-0.042416	2.028447
225.213970	1226.893355	18.529869	-0.042421	2.022914
225.015636	1219.005870	18.534874	-0.042379	2.017385
225.140456	1211.059401	18.539879	-0.042397	2.011833
224.990988	1203.132736	18.544883	-0.042364	2.006252
224.949841	1195.234963	18.549888	-0.042351	2.000686
224.810013	1187.338503	18.554893	-0.042319	1.995096
224.751044	1179.401830	18.559898	-0.042303	1.989469
224.746677	1171.482136	18.564903	-0.042297	1.983845
224.643391	1163.572260	18.569907	-0.042273	1.978201
224.678431	1155.640144	18.574912	-0.042274	1.972540
224.794282	1147.677538	18.579917	-0.042290	1.966849
224.569618	1139.801600	18.584922	-0.042243	1.961167
224.464935	1131.912708	18.589927	-0.042219	1.955473
224.520660	1123.916436	18.594931	-0.042224	1.949701
224.465955	1116.007669	18.599936	-0.042208	1.943964
224.214815	1108.117275	18.604941	-0.042156	1.938202
224.303312	1100.170522	18.609946	-0.042168	1.932418
224.342039	1092.247922	18.614951	-0.042169	1.926630
224.072103	1084.364842	18.619955	-0.042114	1.920819
224.202513	1076.452933	18.624960	-0.042133	1.915013
224.037369	1068.536299	18.629965	-0.042097	1.909154
224.134428	1060.605822	18.634970	-0.042110	1.903295
224.142067	1052.706915	18.639975	-0.042106	1.897432
224.051731	1044.790757	18.644979	-0.042084	1.891526
223.978551	1036.898424	18.649984	-0.042065	1.885622
223.905081	1028.998852	18.654989	-0.042046	1.879694
223.906486	1021.110533	18.659994	-0.042041	1.873764
223.820744	1013.169521	18.664999	-0.042020	1.867765
223.761464	1005.265463	18.670003	-0.042004	1.861778
223.840487	997.360543	18.675008	-0.042013	1.855788
223.650186	989.457230	18.680013	-0.041973	1.849747
223.575945	981.564707	18.685018	-0.041954	1.843709
223.492246	973.691184	18.690023	-0.041933	1.837664
223.549303	965.756092	18.695027	-0.041938	1.831568
223.430939	957.879994	18.700032	-0.041911	1.825477
223.377588	949.973524	18.705037	-0.041896	1.819350
223.397658	942.074537	18.710042	-0.041894	1.813216
223.382624	934.174855	18.715047	-0.041886	1.807057
223.080866	926.319153	18.720051	-0.041825	1.800877
223.332313	918.403142	18.725056	-0.041867	1.794695
223.260538	910.438627	18.730061	-0.041848	1.788414
223.202449	902.557168	18.735066	-0.041832	1.782178
223.111067	894.689421	18.740071	-0.041810	1.775927
222.947644	886.805222	18.745075	-0.041774	1.769632
222.984858	878.921803	18.750080	-0.041776	1.763340
222.874555	871.044368	18.755085	-0.041750	1.757012
222.849738	863.155471	18.760090	-0.041740	1.750663
222.716078	855.289429	18.765095	-0.041710	1.744295
222.549951	847.418244	18.770099	-0.041674	1.737895
222.648406	839.526611	18.775104	-0.041687	1.731489
222.571346	831.631293	18.780109	-0.041667	1.725033
222.466110	823.788236	18.785114	-0.041643	1.718593
222.513830	815.893342	18.790119	-0.041646	1.712105
222.533860	807.979612	18.795123	-0.041645	1.705574
222.492319	800.134410	18.800128	-0.041632	1.699066
222.437231	792.249111	18.805133	-0.041616	1.692498
222.174787	784.403533	18.810138	-0.041562	1.685910
222.236586	776.528181	18.815143	-0.041569	1.679314
222.025651	768.681927	18.820147	-0.041524	1.672680
221.992765	760.807904	18.825152	-0.041513	1.666021
222.032038	752.927615	18.830157	-0.041515	1.659339
221.932438	745.072362	18.835162	-0.041491	1.652632
222.001168	737.192897	18.840167	-0.041499	1.645900
221.884049	729.361579	18.845171	-0.041472	1.639157
221.772246	721.501015	18.850176	-0.041446	1.632361
221.467680	713.627987	18.855181	-0.041384	1.625499
221.660017	705.740065	18.860186	-0.041415	1.618665
221.713057	697.874882	18.865191	-0.041419	1.611802
221.667868	690.009299	18.870195	-0.041406	1.604895
221.418327	682.231067	18.875200	-0.041354	1.598006
221.476498	674.352056	18.880205	-0.041360	1.591042
221.295563	666.527158	18.885210	-0.041321	1.584062
221.177015	658.703611	18.890215	-0.041294	1.577060
221.100563	650.840499	18.895219	-0.041274	1.569998
221.294265	642.985540	18.900224	-0.041305	1.562951
220.993040	635.198286	18.905229	-0.041244	1.555860
220.864159	627.351705	18.910234	-0.041215	1.548709
221.156003	619.458533	18.915239	-0.041264	1.541544
221.110255	611.636426	18.920243	-0.041250	1.534360
220.890050	603.833998	18.925248	-0.041204	1.527135
220.832565	596.008047	18.930253	-0.041188	1.519878
220.838083	588.183582	18.935258	-0.041184	1.512597
220.666788	580.381739	18.940263	-0.041147	1.505275
220.532334	572.581622	18.945267	-0.041117	1.497925
220.618709	564.735767	18.950272	-0.041127	1.490529
220.749175	556.893873	18.955277	-0.041147	1.483107
220.465551	549.141535	18.960282	-0.041089	1.475668
220.520188	541.265511	18.965287	-0.041094	1.468126
220.083825	533.510113	18.970291	-0.041007	1.460584
220.242111	525.687774	18.975296	-0.041031	1.453033
220.190002	517.868163	18.980301	-0.041017	1.445410
220.281465	510.072929	18.985306	-0.041028	1.437795
220.047645	502.316598	18.990311	-0.040980	1.430124
219.896761	494.521644	18.995315	-0.040947	1.422387
220.015347	486.728054	19.000320	-0.040963	1.414654
220.106424	478.912264	19.005325	-0.040975	1.406851
219.961900	471.167505	19.010330	-0.040943	1.399037
220.001607	463.376565	19.015335	-0.040945	1.391164
219.798461	455.613894	19.020339	-0.040903	1.383233
219.596558	447.885636	19.025344	-0.040860	1.375292
219.605693	440.083067	19.030349	-0.040856	1.367264
219.728173	432.307280	19.035354	-0.040874	1.359236
219.598260	424.568278	19.040359	-0.040845	1.351155
219.329834	416.837692	19.045363	-0.040790	1.343010
219.404965	409.079270	19.050368	-0.040798	1.334847
219.256646	401.329750	19.055373	-0.040766	1.326602
219.191482	393.602051	19.060378	-0.040748	1.318345
219.279785	385.759357	19.065383	-0.040760	1.309939
219.145719	377.998241	19.070387	-0.040730	1.301527
219.164688	370.278899	19.075392	-0.040728	1.293134
219.158276	362.543266	19.080397	-0.040722	1.284663
219.132238	354.845990	19.085402	-0.040712	1.276175
218.712130	347.203188	19.090407	-0.040629	1.267617
218.622325	339.490990	19.095411	-0.040607	1.258985
218.891744	331.743566	19.100416	-0.040652	1.250322
218.881837	324.048315	19.105421	-0.040645	1.241604
218.541884	316.412891	19.110426	-0.040576	1.232830
218.429061	308.720241	19.115431	-0.040550	1.223970
218.333597	301.037839	19.120435	-0.040528	1.215062
218.482019	293.331759	19.125440	-0.040550	1.206108
218.315249	285.696441	19.130445	-0.040514	1.197107
218.413737	278.008801	19.135450	-0.040527	1.188030
218.283793	270.376047	19.140455	-0.040498	1.178902
218.001430	262.761207	19.145459	-0.040440	1.169693
217.948947	255.126903	19.150464	-0.040426	1.160435
217.972041	247.464223	19.155469	-0.040425	1.151083
217.915211	239.814571	19.160474	-0.040409	1.141654
217.816207	232.208070	19.165479	-0.040386	1.132191
217.611389	224.616241	19.170483	-0.040343	1.122644
217.458097	217.048831	19.175488	-0.040309	1.113057
217.254334	209.466140	19.180493	-0.040266	1.103356
217.355256	201.854062	19.185498	-0.040280	1.093599
217.324955	194.274564	19.190503	-0.040269	1.083767
217.265819	186.710835	19.195507	-0.040253	1.073859
217.344976	179.127252	19.200512	-0.040263	1.063864
217.099130	171.618091	19.205517	-0.040212	1.053799
217.061226	164.070172	19.210522	-0.040200	1.043632
217.030084	156.562274	19.215527	-0.040189	1.033422
216.992526	149.038897	19.220531	-0.040177	1.023087
216.985966	141.543891	19.225536	-0.040171	1.012694
216.694643	134.093534	19.230541	-0.040112	1.002186
216.617203	126.610098	19.235546	-0.040093	0.991573
216.515124	119.133454	19.240551	-0.040069	0.980848
216.320886	111.700088	19.245555	-0.040028	0.970044
216.101975	104.298754	19.250560	-0.039982	0.959159
216.011005	96.870893	19.255565	-0.039960	0.948143
215.918107	89.473378	19.260570	-0.039938	0.937042
215.813815	82.090403	19.265575	-0.039914	0.925827
215.750555	74.720709	19.270579	-0.039897	0.914507
215.688548	67.360022	19.275584	-0.039880	0.903059
215.471758	60.277081	19.280589	-0.039835	0.891860